Tue Mar 23 10:57:51 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.571841	-0.115444	0.000000	-0.000023	0.721493

0.372827	-0.105970	0.005005	0.000014	0.721442
0.335833	-0.095578	0.010010	0.000020	0.721450
0.550733	-0.134713	0.015014	-0.000020	0.721448
0.490403	-0.126357	0.020019	-0.000008	0.721443
0.341826	-0.096813	0.025024	0.000019	0.721450
0.271224	-0.086707	0.030029	0.000032	0.721445
0.419295	-0.110809	0.035034	0.000005	0.721449
0.404166	-0.107722	0.040038	0.000007	0.721450
0.429068	-0.114778	0.045043	0.000003	0.721445
0.461980	-0.116236	0.050048	-0.000003	0.721454
0.437200	-0.116549	0.055053	0.000001	0.721445
0.384326	-0.105909	0.060058	0.000011	0.721447
0.301630	-0.091031	0.065062	0.000026	0.721448
0.252896	-0.083548	0.070067	0.000035	0.721445
0.271540	-0.083894	0.075072	0.000032	0.721451
0.384761	-0.233721	0.080077	0.000011	0.721196
0.462349	-0.281216	0.085082	-0.000004	0.721130
0.160144	-0.227336	0.090086	0.000052	0.721130
0.247776	-0.245004	0.095091	0.000036	0.721126
0.548765	-0.293834	0.100096	-0.000020	0.721136
0.611026	-0.309405	0.105101	-0.000032	0.721127
0.346823	-0.304295	0.110106	0.000018	0.721045
0.243431	-0.366395	0.115110	0.000037	0.720886
0.479501	-0.411839	0.120115	-0.000007	0.720880
0.464719	-0.402985	0.125120	-0.000004	0.720892
0.461451	-0.407006	0.130125	-0.000004	0.720883
0.319124	-0.442770	0.135130	0.000023	0.720763
0.343142	-0.554476	0.140134	0.000018	0.720551
0.206903	-0.533116	0.145139	0.000043	0.720546
0.273359	-0.542216	0.150144	0.000031	0.720551
0.096215	-0.514286	0.155149	0.000064	0.720544
0.110176	-0.672941	0.160154	0.000061	0.720237
0.156402	-0.682245	0.165158	0.000053	0.720235
0.394289	-0.729397	0.170163	0.000009	0.720225
0.403960	-0.759091	0.175168	0.000007	0.720170
0.329285	-0.882758	0.180173	0.000021	0.719900
0.272502	-0.869800	0.185178	0.000031	0.719906
0.301435	-0.875945	0.190182	0.000026	0.719904
0.151665	-0.974235	0.195187	0.000054	0.719658
0.167934	-1.000846	0.200192	0.000051	0.719611
0.098034	-0.993707	0.205197	0.000064	0.719601
0.163100	-1.108077	0.210202	0.000051	0.719398
0.084146	-1.155709	0.215206	0.000066	0.719277
0.183347	-1.177807	0.220211	0.000048	0.719268
-0.067227	-1.229637	0.225216	0.000094	0.719078
-0.029482	-1.294619	0.230221	0.000087	0.718963
0.185211	-1.329767	0.235226	0.000047	0.718969
0.288286	-1.480112	0.240230	0.000028	0.718709
-0.017913	-1.457414	0.245235	0.000085	0.718646
0.156808	-1.516871	0.250240	0.000053	0.718590
0.025500	-1.612291	0.255245	0.000077	0.718355
-0.158333	-1.579164	0.260250	0.000111	0.718356
-0.049294	-1.708139	0.265254	0.000091	0.718140
-0.039874	-1.771675	0.270259	0.000089	0.718018
0.089429	-1.832381	0.275264	0.000065	0.717943
0.009456	-1.938611	0.280269	0.000080	0.717705
0.122059	-1.956574	0.285274	0.000059	0.717710
-0.107793	-2.075537	0.290278	0.000102	0.717394
-0.218200	-2.063455	0.295283	0.000122	0.717379
-0.478735	-2.119445	0.300288	0.000171	0.717176
-0.459032	-2.169030	0.305293	0.000167	0.717085
-0.432389	-2.245874	0.310298	0.000162	0.716942
-0.626460	-2.302361	0.315302	0.000198	0.716762
-1.955446	-2.084565	0.320307	0.000446	0.716725
-2.395031	-2.141907	0.325312	0.000527	0.716457
-2.354639	-2.152809	0.330317	0.000520	0.716449
-2.756802	-2.121853	0.335322	0.000595	0.716369
-3.405652	-2.123301	0.340326	0.000715	0.716137
-3.537912	-2.103688	0.345331	0.000740	0.716129
-3.551287	-2.102924	0.350336	0.000742	0.716126
-4.272990	-2.097417	0.355341	0.000877	0.715882
-4.266950	-2.097196	0.360346	0.000876	0.715885
-4.058631	-2.134145	0.365350	0.000837	0.715886
-4.393677	-2.187146	0.370355	0.000899	0.715662
-5.494609	-2.046481	0.375360	0.001104	0.715552
-5.303394	-2.084202	0.380365	0.001068	0.715545
-5.327942	-2.079046	0.385370	0.001073	0.715547
-5.454323	-2.157037	0.390374	0.001096	0.715348
-6.592696	-2.015102	0.395379	0.001308	0.715227
-6.087245	-2.100805	0.400384	0.001214	0.715236
-6.164326	-2.090148	0.405389	0.001228	0.715230
-6.405340	-2.088052	0.410394	0.001273	0.715149
-6.819100	-2.132255	0.415398	0.001350	0.714915
-7.119250	-2.083475	0.420403	0.001406	0.714906
-7.065745	-2.088763	0.425408	0.001396	0.714914
-7.168241	-2.075857	0.430413	0.001415	0.714904
-7.177217	-2.145380	0.435418	0.001417	0.714762
-8.343247	-2.014375	0.440422	0.001634	0.714610
-8.121528	-2.058508	0.445427	0.001593	0.714601
-7.821458	-2.106851	0.450432	0.001537	0.714611
-8.379959	-2.009536	0.455437	0.001641	0.714607
-8.312772	-2.020721	0.460442	0.001628	0.714609
-8.001636	-2.222508	0.465446	0.001570	0.714318
-8.859212	-2.092108	0.470451	0.001730	0.714274
-9.327127	-2.001773	0.475456	0.001817	0.714288
-9.160460	-2.036688	0.480461	0.001786	0.714277
-9.230919	-2.024220	0.485466	0.001799	0.714277
-8.816156	-2.115818	0.490470	0.001722	0.714242
-9.899933	-2.061517	0.495475	0.001923	0.713967
-9.680073	-2.096562	0.500480	0.001882	0.713975
-10.078801	-2.028053	0.505485	0.001956	0.713970
-10.098656	-2.024717	0.510490	0.001960	0.713970
-9.526531	-2.123176	0.515494	0.001854	0.713977
-10.293003	-1.991479	0.520499	0.001996	0.713967
-10.414810	-2.096346	0.525504	0.002019	0.713715
-10.657075	-2.085612	0.530509	0.002064	0.713651
-10.675050	-2.080452	0.535514	0.002067	0.713655
-10.667128	-2.079904	0.540518	0.002066	0.713659
-10.871333	-2.047928	0.545523	0.002104	0.713650
-10.440298	-2.118669	0.550528	0.002023	0.713662
-10.815154	-2.143368	0.555533	0.002093	0.713481
-12.208553	-1.956124	0.560538	0.002352	0.713359
-11.487248	-2.081794	0.565542	0.002218	0.713365
-11.534539	-2.076629	0.570547	0.002227	0.713359
-11.648670	-2.052261	0.575552	0.002248	0.713367
-11.515783	-2.080370	0.580557	0.002223	0.713358
-11.667846	-2.051599	0.585562	0.002252	0.713362
-12.154010	-2.129992	0.590566	0.002342	0.713033
-12.618378	-2.053037	0.595571	0.002429	0.713022
-12.694541	-2.036101	0.600576	0.002443	0.713029
-12.690801	-2.038535	0.605581	0.002442	0.713025
-12.628049	-2.050070	0.610586	0.002430	0.713025
-12.344326	-2.097832	0.615590	0.002377	0.713030
-12.623879	-2.072933	0.620595	0.002429	0.712981
-13.549987	-2.040410	0.625600	0.002602	0.712717
-13.100012	-2.122965	0.630605	0.002518	0.712712
-13.390218	-2.070800	0.635610	0.002572	0.712713
-13.447654	-2.057985	0.640614	0.002583	0.712719
-13.909976	-1.981781	0.645619	0.002669	0.712706
-13.437826	-2.060840	0.650624	0.002581	0.712717
-13.388311	-2.085576	0.655629	0.002571	0.712685
-14.700268	-2.000824	0.660634	0.002816	0.712388
-14.558333	-2.023331	0.665638	0.002789	0.712394
-14.737898	-1.996125	0.670643	0.002822	0.712384
-14.547003	-2.024770	0.675648	0.002787	0.712395
-14.446810	-2.046070	0.680653	0.002768	0.712388
-14.614868	-2.015742	0.685658	0.002799	0.712389
-14.379039	-2.054977	0.690662	0.002756	0.712395
-14.697380	-2.060312	0.695667	0.002815	0.712271
-15.322298	-2.035766	0.700672	0.002931	0.712099
-15.167728	-2.067887	0.705677	0.002902	0.712089
-15.678423	-1.974404	0.710682	0.002997	0.712095
-15.301544	-2.041079	0.715686	0.002927	0.712096
-15.178176	-2.067838	0.720691	0.002904	0.712086
-15.347217	-2.031697	0.725696	0.002935	0.712098
-15.662093	-2.027051	0.730701	0.002994	0.711996
-16.138196	-2.058019	0.735706	0.003083	0.711765
-16.048149	-2.072578	0.740710	0.003066	0.711768
-16.776005	-1.948114	0.745715	0.003201	0.711758
-16.359195	-2.016388	0.750720	0.003124	0.711770
-16.159777	-2.055871	0.755725	0.003086	0.711762
-16.696203	-1.960073	0.760730	0.003186	0.711762
-16.345537	-2.019106	0.765734	0.003121	0.711769
-16.796625	-2.077807	0.770739	0.003205	0.711492
-17.348205	-1.995737	0.775744	0.003308	0.711460
-17.299518	-2.006605	0.780749	0.003298	0.711456
-16.922981	-2.072793	0.785754	0.003228	0.711457
-17.122203	-2.035738	0.790758	0.003265	0.711461
-17.422751	-1.987360	0.795763	0.003321	0.711450
-16.982526	-2.062899	0.800768	0.003239	0.711456
-17.512195	-2.092128	0.805773	0.003338	0.711210
-18.481725	-1.958108	0.810778	0.003518	0.711132
-17.815650	-2.072442	0.815782	0.003394	0.711141
-17.796599	-2.080532	0.820787	0.003391	0.711132
-18.161031	-2.010876	0.825792	0.003458	0.711141
-18.428759	-1.966074	0.830797	0.003508	0.711136
-18.168370	-2.012548	0.835802	0.003460	0.711136
-18.046564	-2.106463	0.840806	0.003437	0.710992
-19.230782	-1.957863	0.845811	0.003657	0.710867
-18.646194	-2.057956	0.850816	0.003549	0.710875
-18.640232	-2.062579	0.855821	0.003547	0.710868
-18.981955	-2.001503	0.860826	0.003611	0.710869
-18.726213	-2.044180	0.865830	0.003563	0.710875
-18.583236	-2.074269	0.870835	0.003537	0.710865
-19.108954	-2.139486	0.875840	0.003635	0.710548
-19.721876	-2.037395	0.880845	0.003749	0.710534
-19.940019	-2.001540	0.885850	0.003789	0.710528
-19.475663	-2.079630	0.890854	0.003703	0.710538
-19.866602	-2.013339	0.895859	0.003775	0.710531
-19.696421	-2.039875	0.900864	0.003744	0.710539
-19.522216	-2.114863	0.905869	0.003711	0.710451
-20.672185	-2.027446	0.910874	0.003925	0.710216
-20.472631	-2.060936	0.915878	0.003888	0.710220
-20.782253	-2.008779	0.920883	0.003946	0.710214
-20.418436	-2.070170	0.925888	0.003878	0.710221
-20.725744	-2.017645	0.930893	0.003935	0.710217
-20.571583	-2.046092	0.935898	0.003906	0.710215
-20.277122	-2.155527	0.940902	0.003852	0.710101
-21.798790	-1.991161	0.945907	0.004135	0.709888
-21.330158	-2.070919	0.950912	0.004047	0.709895
-21.277248	-2.081599	0.955917	0.004038	0.709893
-21.676111	-2.009948	0.960922	0.004112	0.709894
-21.284753	-2.076835	0.965926	0.004039	0.709900
-21.597916	-2.025332	0.970931	0.004097	0.709892
-21.462323	-2.106473	0.975936	0.004072	0.709778
-22.414248	-2.026676	0.980941	0.004249	0.709598
-22.057197	-2.091588	0.985946	0.004183	0.709596
-22.069165	-2.085792	0.990950	0.004185	0.709603
-22.797882	-1.959813	0.995955	0.004320	0.709595
-22.128970	-2.076314	1.000960	0.004196	0.709601
-22.022331	-2.096684	1.005965	0.004176	0.709598
-22.435087	-2.136997	1.010970	0.004253	0.709370
-23.443279	-2.005943	1.015974	0.004440	0.709273
-23.479284	-2.005770	1.020979	0.004447	0.709261
-22.898046	-2.106691	1.025984	0.004339	0.709266
-23.150295	-2.062644	1.030989	0.004386	0.709265
-23.247724	-2.046106	1.035994	0.004404	0.709263
-23.035439	-2.080038	1.040998	0.004364	0.709271
-23.517258	-2.091927	1.046003	0.004454	0.709075
-24.317935	-2.005308	1.051008	0.004603	0.708963
-23.902206	-2.080716	1.056013	0.004525	0.708961
-24.218800	-2.025826	1.061018	0.004584	0.708958
-24.351256	-1.998953	1.066022	0.004609	0.708964
-24.113489	-2.045456	1.071027	0.004565	0.708956
-23.728305	-2.111251	1.076032	0.004493	0.708962
-24.247163	-2.103286	1.081037	0.004589	0.708793
-25.405975	-1.973314	1.086042	0.004805	0.708639
-24.744957	-2.086277	1.091046	0.004682	0.708649
-24.901072	-2.063721	1.096051	0.004711	0.708639
-25.028905	-2.038336	1.101056	0.004735	0.708644
-24.860259	-2.070768	1.106061	0.004703	0.708639
-25.200894	-2.011864	1.111066	0.004767	0.708636
-25.048787	-2.092416	1.116070	0.004738	0.708529
-25.997961	-2.011917	1.121075	0.004915	0.708351
-25.511709	-2.095883	1.126080	0.004825	0.708357
-25.842805	-2.037977	1.131085	0.004886	0.708355
-26.108376	-1.993654	1.136090	0.004935	0.708349
-25.443126	-2.108934	1.141094	0.004812	0.708355
-26.060133	-2.003505	1.146099	0.004926	0.708346
-25.951101	-2.100652	1.151104	0.004906	0.708191
-26.800259	-2.036916	1.156109	0.005064	0.708015
-26.660627	-2.062114	1.161114	0.005038	0.708015
-26.784242	-2.035925	1.166118	0.005061	0.708023
-26.999480	-2.003917	1.171123	0.005101	0.708010
-26.597964	-2.071658	1.176128	0.005026	0.708018
-26.859951	-2.026960	1.181133	0.005075	0.708014
-27.045386	-2.043187	1.186138	0.005110	0.707915
-27.482602	-2.068540	1.191142	0.005191	0.707708
-27.628697	-2.048344	1.196147	0.005218	0.707697
-27.616500	-2.048070	1.201152	0.005216	0.707702
-27.569449	-2.056498	1.206157	0.005207	0.707702
-27.656466	-2.042240	1.211162	0.005223	0.707699
-27.681537	-2.034547	1.216166	0.005228	0.707706
-27.704692	-2.067807	1.221171	0.005232	0.707631
-28.197245	-2.104368	1.226176	0.005324	0.707381
-28.549828	-2.043248	1.231181	0.005389	0.707378
-28.955422	-1.973148	1.236186	0.005465	0.707374
-28.503996	-2.050763	1.241190	0.005381	0.707380
-28.606298	-2.036929	1.246195	0.005400	0.707371
-28.780488	-2.000642	1.251200	0.005432	0.707381
-28.575572	-2.038253	1.256205	0.005394	0.707379
-29.133302	-2.081611	1.261210	0.005498	0.707093
-29.498520	-2.019443	1.266214	0.005566	0.707087
-29.952446	-1.942904	1.271219	0.005650	0.707078
-29.281421	-2.057558	1.276224	0.005525	0.707088
-29.134881	-2.085893	1.281229	0.005498	0.707084
-29.675785	-1.990744	1.286234	0.005598	0.707082
-29.290947	-2.055950	1.291238	0.005527	0.707088
-29.763078	-2.106537	1.296243	0.005615	0.706818
-30.416071	-2.019924	1.301248	0.005736	0.706758
-30.332430	-2.035223	1.306253	0.005721	0.706758
-30.044088	-2.089839	1.311258	0.005667	0.706751
-30.310329	-2.038703	1.316262	0.005716	0.706759
-30.505663	-2.008285	1.321267	0.005753	0.706750
-30.186964	-2.062834	1.326272	0.005693	0.706755
-30.709296	-2.106385	1.331277	0.005791	0.706480
-31.531437	-1.978232	1.336282	0.005943	0.706443
-31.135352	-2.042149	1.341286	0.005870	0.706457
-30.821810	-2.105100	1.346291	0.005811	0.706443
-31.282982	-2.020583	1.351296	0.005897	0.706447
-31.185996	-2.039581	1.356301	0.005879	0.706444
-31.121272	-2.051431	1.361306	0.005867	0.706443
-31.791416	-2.075210	1.366310	0.005992	0.706156
-32.425616	-1.977203	1.371315	0.006110	0.706125
-32.137617	-2.025587	1.376320	0.006056	0.706131
-31.962023	-2.055722	1.381325	0.006023	0.706134
-32.441569	-1.974294	1.386330	0.006112	0.706126
-32.165764	-2.019961	1.391334	0.006061	0.706133
-32.096583	-2.036525	1.396339	0.006048	0.706124
-32.414717	-2.050652	1.401344	0.006107	0.705982
-33.351945	-1.942861	1.406349	0.006282	0.705863
-33.036985	-2.000435	1.411354	0.006223	0.705860
-32.705570	-2.054852	1.416358	0.006161	0.705870
-33.299744	-1.954465	1.421363	0.006272	0.705859
-32.925715	-2.018184	1.426368	0.006202	0.705865
-32.801653	-2.040921	1.431373	0.006179	0.705863
-33.187003	-2.041642	1.436378	0.006251	0.705724
-33.808210	-2.027572	1.441382	0.006366	0.705530
-33.464704	-2.093260	1.446387	0.006303	0.705521
-33.778620	-2.034367	1.451392	0.006361	0.705527
-33.986849	-1.996016	1.456397	0.006400	0.705529
-33.910941	-2.013001	1.461402	0.006385	0.705522
-33.509604	-2.079186	1.466406	0.006311	0.705533
-34.259896	-2.052198	1.471411	0.006450	0.705318
-35.077313	-1.957052	1.476416	0.006602	0.705217
-34.344875	-2.088845	1.481421	0.006466	0.705214
-34.899067	-1.994063	1.486426	0.006569	0.705206
-35.032168	-1.967320	1.491430	0.006594	0.705212
-34.824755	-2.006347	1.496435	0.006555	0.705208
-34.583502	-2.045825	1.501440	0.006510	0.705216
-34.918346	-2.049976	1.506445	0.006573	0.705087
-35.840763	-1.984872	1.511450	0.006744	0.704887
-35.299523	-2.077397	1.516454	0.006644	0.704895
-36.099833	-1.938393	1.521459	0.006792	0.704888
-35.969368	-1.960490	1.526464	0.006768	0.704890
-35.297366	-2.080312	1.531469	0.006643	0.704890
-35.738909	-2.003125	1.536474	0.006725	0.704887
-35.596146	-2.067429	1.541478	0.006699	0.704809
-36.276127	-2.057499	1.546483	0.006825	0.704585
-36.147981	-2.077711	1.551488	0.006801	0.704590
-36.658350	-1.986473	1.556493	0.006896	0.704591
-36.571199	-2.004335	1.561498	0.006880	0.704586
-35.812777	-2.135691	1.566502	0.006739	0.704594
-36.794307	-1.964149	1.571507	0.006921	0.704587
-36.778424	-2.061802	1.576512	0.006918	0.704396
-37.164058	-2.059219	1.581517	0.006990	0.704263
-37.250971	-2.046324	1.586522	0.007006	0.704258
-37.409917	-2.013003	1.591526	0.007036	0.704268
-37.354707	-2.028422	1.596531	0.007025	0.704257
-37.107698	-2.070288	1.601536	0.006979	0.704261
-36.968867	-2.093800	1.606541	0.006954	0.704264
-37.983650	-2.054080	1.611546	0.007142	0.703979
-37.983473	-2.063710	1.616550	0.007142	0.703960
-38.402129	-1.994039	1.621555	0.007220	0.703950
-38.316771	-2.006705	1.626560	0.007204	0.703955
-38.134451	-2.039673	1.631565	0.007170	0.703954
-38.403785	-1.993601	1.636570	0.007220	0.703951
-37.966004	-2.067734	1.641574	0.007139	0.703959
-38.457107	-2.113561	1.646579	0.007230	0.703690
-39.222484	-2.003658	1.651584	0.007373	0.703636
-39.362291	-1.977001	1.656589	0.007399	0.703640
-39.025684	-2.040295	1.661594	0.007336	0.703633
-38.455387	-2.136855	1.666598	0.007230	0.703644
-39.119282	-2.022072	1.671603	0.007353	0.703636
-39.398041	-1.971302	1.676608	0.007405	0.703639
-39.406537	-2.096714	1.681613	0.007407	0.703383
-39.959509	-2.017471	1.686618	0.007510	0.703344
-39.840682	-2.035991	1.691622	0.007487	0.703349
-40.040369	-2.004650	1.696627	0.007525	0.703341
-40.000020	-2.010610	1.701632	0.007517	0.703343
-39.567653	-2.086645	1.706637	0.007437	0.703345
-40.161436	-1.988531	1.711642	0.007547	0.703330
-40.561939	-2.074215	1.716646	0.007622	0.703013
-40.834491	-2.029303	1.721651	0.007672	0.703005
-41.242452	-1.956620	1.726656	0.007748	0.703005
-40.549137	-2.077630	1.731661	0.007619	0.703011
-41.069478	-1.988043	1.736666	0.007716	0.703004
-41.036813	-1.989196	1.741670	0.007710	0.703014
-41.009163	-1.999190	1.746675	0.007705	0.703004
-40.927761	-2.115870	1.751680	0.007689	0.702797
-41.932853	-1.984235	1.756685	0.007876	0.702701
-41.866931	-1.997960	1.761690	0.007864	0.702697
-41.433718	-2.071641	1.766694	0.007783	0.702705
-41.828858	-2.006378	1.771699	0.007857	0.702694
-41.975824	-1.978522	1.776704	0.007884	0.702698
-41.627765	-2.040111	1.781709	0.007819	0.702699
-42.032349	-2.075126	1.786714	0.007895	0.702482
-42.559033	-2.031685	1.791718	0.007993	0.702380
-42.529154	-2.040528	1.796723	0.007987	0.702373
-42.493385	-2.046176	1.801728	0.007980	0.702375
-42.726855	-2.003362	1.806733	0.008024	0.702377
-42.870625	-1.981248	1.811738	0.008051	0.702370
-42.687515	-2.009767	1.816742	0.008016	0.702379
-42.831825	-2.070062	1.821747	0.008043	0.702205
-43.842145	-1.952259	1.826752	0.008231	0.702079
-43.267218	-2.053178	1.831757	0.008124	0.702082
-43.472620	-2.019689	1.836762	0.008162	0.702076
-43.682334	-1.978217	1.841766	0.008201	0.702084
-43.772851	-1.965787	1.846771	0.008218	0.702077
-43.526182	-2.008687	1.851776	0.008172	0.702079
-43.384988	-2.104222	1.856781	0.008146	0.701937
-44.838791	-1.939409	1.861786	0.008417	0.701746
-44.099721	-2.066664	1.866790	0.008279	0.701755
-44.357460	-2.022994	1.871795	0.008327	0.701750
-44.727941	-1.956832	1.876800	0.008396	0.701751
-44.341622	-2.023936	1.881805	0.008324	0.701754
-44.561216	-1.989071	1.886810	0.008365	0.701746
-44.555784	-2.027482	1.891814	0.008364	0.701670
-45.531571	-1.966041	1.896819	0.008545	0.701442
-45.320277	-2.002251	1.901824	0.008506	0.701445
-45.202789	-2.022624	1.906829	0.008484	0.701447
-45.623879	-1.951832	1.911834	0.008562	0.701438
-45.060109	-2.047068	1.916838	0.008457	0.701449
-45.156501	-2.034628	1.921843	0.008475	0.701439
-45.460908	-1.996124	1.926848	0.008532	0.701408
-45.679617	-2.095232	1.931853	0.008573	0.701128
-46.009266	-2.037889	1.936858	0.008634	0.701125
-46.319327	-1.978337	1.941862	0.008692	0.701134
-46.156530	-2.009639	1.946867	0.008661	0.701129
-45.892658	-2.056650	1.951872	0.008612	0.701129
-46.004602	-2.036002	1.956877	0.008633	0.701131
-46.478308	-2.009061	1.961882	0.008721	0.701014
-47.027916	-1.976777	1.966886	0.008823	0.700881
-46.693189	-2.039118	1.971891	0.008761	0.700876
-46.911718	-2.000468	1.976896	0.008802	0.700876
-46.821394	-2.016192	1.981901	0.008785	0.700876
-46.956971	-1.995027	1.986906	0.008810	0.700870
-46.657751	-2.043644	1.991910	0.008754	0.700880
-47.191452	-2.080245	1.996915	0.008854	0.700613
-47.951164	-1.981196	2.001920	0.008995	0.700539

-47.836633	-2.001162	2.011917	0.008973	0.700540
-47.791677	-2.011306	2.021914	0.008965	0.700536
-47.801076	-2.009330	2.031910	0.008967	0.700537
-47.747543	-2.017303	2.041907	0.008957	0.700540
-47.686717	-2.027309	2.051904	0.008945	0.700542
-47.921844	-1.987245	2.061901	0.008989	0.700539
-47.781933	-2.011082	2.071898	0.008963	0.700541
-47.889565	-1.991938	2.081894	0.008983	0.700541
-47.711681	-2.022237	2.091891	0.008949	0.700544
-47.690230	-2.026340	2.101888	0.008945	0.700544
-47.751999	-2.017609	2.111885	0.008957	0.700539
-47.755673	-2.017464	2.121882	0.008957	0.700539
-47.863113	-1.998971	2.131878	0.008977	0.700537
-47.451234	-2.012175	2.141875	0.008901	0.700660
-46.860473	-2.008834	2.151872	0.008790	0.700880
-46.982241	-1.988520	2.161869	0.008813	0.700877
-46.867019	-2.009226	2.171866	0.008791	0.700877
-46.900050	-2.002459	2.181862	0.008798	0.700879
-46.438658	-2.010304	2.191859	0.008712	0.701030
-46.202117	-2.003617	2.201856	0.008667	0.701129
-45.989854	-2.043900	2.211853	0.008628	0.701125
-46.284424	-1.990232	2.221850	0.008683	0.701127
-45.657791	-1.986765	2.231846	0.008566	0.701361
-45.160242	-2.034575	2.241843	0.008473	0.701444
-45.115939	-2.041787	2.251840	0.008465	0.701445
-45.352240	-1.999667	2.261837	0.008509	0.701445
-44.492133	-2.012363	2.271834	0.008348	0.701730
-44.692713	-1.966458	2.281830	0.008386	0.701751
-44.087153	-2.074813	2.291827	0.008273	0.701750
-44.568046	-1.932753	2.301824	0.008362	0.701865
-43.410456	-2.034356	2.311821	0.008147	0.702077
-43.785951	-1.967538	2.321818	0.008216	0.702077
-43.651264	-1.990206	2.331814	0.008191	0.702080
-42.778918	-2.007147	2.341811	0.008029	0.702360
-42.727580	-2.009081	2.351808	0.008019	0.702375
-42.851386	-1.986709	2.361805	0.008042	0.702376
-42.451753	-1.983330	2.371802	0.007968	0.702527
-41.718047	-2.030790	2.381798	0.007831	0.702695
-41.707811	-2.031734	2.391795	0.007829	0.702697
-41.892403	-1.999144	2.401792	0.007863	0.702697
-41.078451	-2.016255	2.411789	0.007712	0.702956
-41.258034	-1.957754	2.421786	0.007745	0.703009
-40.808429	-2.038028	2.431782	0.007661	0.703009
-40.687488	-2.008223	2.441779	0.007638	0.703113
-40.142662	-1.988886	2.451776	0.007537	0.703349
-39.956753	-2.022112	2.461773	0.007502	0.703349
-39.930775	-2.028608	2.471770	0.007497	0.703345
-39.578298	-1.989652	2.481766	0.007432	0.703551
-39.197282	-2.013638	2.491763	0.007361	0.703640
-39.369090	-1.982478	2.501760	0.007392	0.703641
-39.095431	-1.973032	2.511757	0.007341	0.703758
-38.462687	-1.989936	2.521754	0.007223	0.703952
-38.400920	-2.000760	2.531750	0.007212	0.703953
-38.277577	-2.021980	2.541747	0.007189	0.703954
-37.712375	-1.976711	2.551744	0.007083	0.704249
-37.286753	-2.046308	2.561741	0.007004	0.704262
-37.432897	-2.020576	2.571738	0.007031	0.704261
-37.409364	-1.965714	2.581734	0.007027	0.704381
-36.294229	-2.058234	2.591731	0.006819	0.704595
-36.657384	-1.992968	2.601728	0.006887	0.704596
-36.383154	-2.043446	2.611725	0.006835	0.704593
-36.131243	-1.967908	2.621722	0.006788	0.704836
-35.620639	-2.031349	2.631718	0.006693	0.704892
-35.787991	-2.000093	2.641715	0.006724	0.704895
-35.565078	-1.977337	2.651712	0.006683	0.705021
-34.543528	-2.060906	2.661709	0.006493	0.705220
-35.036135	-1.974626	2.671706	0.006584	0.705217
-34.799569	-2.017420	2.681702	0.006540	0.705216
-34.140396	-1.999449	2.691699	0.006417	0.705488
-33.839113	-2.033627	2.701696	0.006361	0.705528
-33.941908	-2.015701	2.711693	0.006380	0.705527
-33.888439	-1.971655	2.721690	0.006370	0.705635
-32.974050	-2.020372	2.731686	0.006200	0.705865
-33.165717	-1.985830	2.741683	0.006235	0.705866
-33.016250	-2.012983	2.751680	0.006207	0.705865
-32.330766	-2.020472	2.761677	0.006080	0.706096
-32.355704	-1.999947	2.771674	0.006084	0.706129
-32.119071	-2.043178	2.781670	0.006040	0.706127
-32.046770	-1.992645	2.791667	0.006026	0.706255
-31.100827	-2.065886	2.801664	0.005850	0.706446
-31.412286	-2.012328	2.811661	0.005908	0.706443
-31.521550	-1.994535	2.821658	0.005928	0.706439
-30.527239	-2.024406	2.831654	0.005743	0.706736
-30.391864	-2.039438	2.841651	0.005718	0.706754
-30.450227	-2.030484	2.851648	0.005729	0.706751
-30.290541	-1.994337	2.861645	0.005699	0.706881
-29.470220	-2.042564	2.871642	0.005546	0.707078
-29.345966	-2.063860	2.881638	0.005523	0.707080
-29.703561	-1.999827	2.891635	0.005589	0.707081
-28.758970	-2.045606	2.901632	0.005413	0.707327
-28.970890	-1.984215	2.911629	0.005453	0.707375
-28.786080	-2.018482	2.921626	0.005418	0.707372
-28.448207	-2.005618	2.931622	0.005355	0.707519
-27.590229	-2.067662	2.941619	0.005195	0.707702
-27.837706	-2.024191	2.951616	0.005241	0.707701
-27.877937	-2.016796	2.961613	0.005249	0.707701
-27.203751	-1.996887	2.971610	0.005123	0.707982
-26.712415	-2.068319	2.981606	0.005031	0.708015
-26.897445	-2.034107	2.991603	0.005066	0.708017
-26.491164	-2.067816	3.001600	0.004990	0.708095
-25.806090	-2.060406	3.011597	0.004862	0.708355
-25.582332	-2.100209	3.021594	0.004821	0.708355
-25.791241	-2.064588	3.031590	0.004860	0.708352
-25.795743	-2.016340	3.041587	0.004860	0.708448
-25.027914	-2.055905	3.051584	0.004717	0.708643
-25.256593	-2.015202	3.061581	0.004760	0.708643
-24.978533	-2.065032	3.071578	0.004708	0.708642
-24.369131	-2.026663	3.081574	0.004594	0.708937
-24.293717	-2.029104	3.091571	0.004580	0.708959
-24.038640	-2.073159	3.101568	0.004533	0.708962
-24.014833	-2.012232	3.111565	0.004528	0.709093
-23.363764	-2.040966	3.121562	0.004407	0.709268
-23.562632	-2.006436	3.131558	0.004444	0.709266
-23.515356	-1.989880	3.141555	0.004435	0.709316
-22.612940	-2.008024	3.151552	0.004267	0.709602
-22.693557	-1.996323	3.161549	0.004282	0.709597
-22.424912	-2.044824	3.171546	0.004231	0.709596
-22.005133	-2.000159	3.181542	0.004153	0.709835
-21.839109	-1.998683	3.191539	0.004122	0.709897
-21.649464	-2.032129	3.201536	0.004087	0.709898
-21.659834	-1.962833	3.211533	0.004089	0.710033
-20.587022	-2.061657	3.221530	0.003889	0.710218
-20.795190	-2.023323	3.231526	0.003927	0.710220
-20.809067	-2.020740	3.241523	0.003930	0.710221
-20.073732	-2.012747	3.251520	0.003793	0.710499
-19.870020	-2.031527	3.261517	0.003755	0.710534
-19.851015	-2.035547	3.271514	0.003751	0.710533
-19.972672	-1.949763	3.281510	0.003774	0.710661
-18.912805	-2.031120	3.291507	0.003576	0.710876
-19.012009	-2.014900	3.301504	0.003595	0.710873
-19.161408	-1.987781	3.311501	0.003622	0.710874
-18.204958	-2.034037	3.321498	0.003444	0.711122
-18.512566	-1.968747	3.331494	0.003501	0.711143
-18.265638	-2.013453	3.341491	0.003455	0.711142
-17.857505	-1.995569	3.351488	0.003379	0.711323
-17.321541	-2.023192	3.361485	0.003279	0.711459
-17.362658	-2.015717	3.371482	0.003287	0.711459
-17.537372	-1.962898	3.381478	0.003319	0.711503
-16.570912	-2.002116	3.391475	0.003139	0.711768
-16.436191	-2.026281	3.401472	0.003114	0.711768
-16.733387	-1.974556	3.411469	0.003169	0.711766
-15.887850	-1.991824	3.421466	0.003012	0.712032
-15.911413	-1.957486	3.431462	0.003016	0.712092
-15.496374	-2.030531	3.441459	0.002939	0.712094
-15.661097	-1.943008	3.451456	0.002969	0.712210
-14.587567	-2.043751	3.461453	0.002770	0.712391
-14.938832	-1.982711	3.471450	0.002835	0.712388
-14.924390	-1.983761	3.481446	0.002832	0.712391
-13.961313	-1.996764	3.491443	0.002653	0.712707
-14.110004	-1.965849	3.501440	0.002680	0.712716
-13.802517	-2.021849	3.511437	0.002623	0.712714
-13.701605	-1.960793	3.521434	0.002604	0.712871
-12.664998	-2.067700	3.531430	0.002411	0.713026
-12.894928	-2.026197	3.541427	0.002454	0.713027
-12.729468	-2.054934	3.551424	0.002423	0.713029
-12.329572	-2.009205	3.561421	0.002348	0.713262
-11.967980	-2.023195	3.571418	0.002281	0.713362
-11.802485	-2.051779	3.581414	0.002250	0.713364
-11.797115	-2.051918	3.591411	0.002249	0.713366
-11.305757	-2.018296	3.601408	0.002157	0.713607
-10.735931	-2.093519	3.611405	0.002051	0.713660
-11.046203	-2.038964	3.621402	0.002109	0.713659
-10.763563	-2.089083	3.631398	0.002056	0.713659
-10.187977	-2.032552	3.641395	0.001949	0.713976
-9.479710	-2.157699	3.651392	0.001817	0.713978
-9.886075	-2.086697	3.661389	0.001892	0.713975
-9.887725	-2.085938	3.671386	0.001893	0.713976
-9.150959	-2.063430	3.681382	0.001755	0.714282
-8.858674	-2.113298	3.691379	0.001701	0.714287
-8.864245	-2.112312	3.701376	0.001702	0.714287
-8.785403	-2.114602	3.711373	0.001687	0.714310
-8.380204	-2.034097	3.721370	0.001611	0.714614
-7.927776	-2.115792	3.731366	0.001527	0.714612
-7.960396	-2.109792	3.741363	0.001533	0.714612
-7.873200	-2.062717	3.751360	0.001517	0.714737
-7.015750	-2.125742	3.761357	0.001357	0.714915
-7.339138	-2.069920	3.771354	0.001417	0.714912
-7.119868	-2.109888	3.781350	0.001376	0.714910
-6.252023	-2.137839	3.791347	0.001215	0.715162
-6.342396	-2.085042	3.801344	0.001231	0.715234
-6.140998	-2.121432	3.811341	0.001194	0.715234
-6.408866	-2.061046	3.821338	0.001243	0.715259
-5.397990	-2.095175	3.831334	0.001055	0.715549
-5.181256	-2.132878	3.841331	0.001015	0.715551
-5.272451	-2.115972	3.851328	0.001032	0.715552
-5.146119	-2.065611	3.861325	0.001008	0.715697
-4.408316	-2.101118	3.871322	0.000871	0.715887
-4.334804	-2.113074	3.881318	0.000857	0.715889
-4.459061	-2.090596	3.891315	0.000880	0.715890
-3.824194	-2.111368	3.901312	0.000762	0.716073
-3.639424	-2.109420	3.911309	0.000727	0.716143
-3.764424	-2.090635	3.921306	0.000750	0.716136
-3.477242	-2.088108	3.931302	0.000697	0.716242
-2.892065	-2.085697	3.941299	0.000588	0.716454
-2.949031	-2.075321	3.951296	0.000598	0.716454
-2.875043	-2.077299	3.961293	0.000584	0.716477
-2.298328	-2.037344	3.971290	0.000477	0.716759
-2.267824	-2.042783	3.981286	0.000471	0.716760
-1.940979	-2.099616	3.991283	0.000410	0.716762
-1.996824	-1.949277	4.001280	0.000420	0.717041
-1.594114	-1.995569	4.011277	0.000345	0.717091
-1.730218	-1.970310	4.021274	0.000370	0.717093
-1.612714	-1.845758	4.031270	0.000348	0.717381
-0.953497	-1.961462	4.041267	0.000226	0.717385
-1.350570	-1.817537	4.051264	0.000299	0.717530
-0.903153	-1.807542	4.061261	0.000216	0.717707
-0.984086	-1.779736	4.071258	0.000231	0.717734
-1.005257	-1.630514	4.081254	0.000235	0.718021
-0.788290	-1.665717	4.091251	0.000194	0.718028
-0.947561	-1.472180	4.101248	0.000224	0.718355
-0.676673	-1.497832	4.111245	0.000173	0.718400
-0.487353	-1.406974	4.121242	0.000138	0.718646
-0.632103	-1.319969	4.131238	0.000165	0.718767
-0.220089	-1.294044	4.141235	0.000088	0.718963
-0.501448	-1.135871	4.151232	0.000140	0.719177
-0.316512	-1.091165	4.161229	0.000105	0.719330
-0.254995	-0.963792	4.171226	0.000094	0.719603
-0.519911	-0.813369	4.181222	0.000143	0.719807
-0.206838	-0.758970	4.191219	0.000084	0.720024
-0.322128	-0.623785	4.201216	0.000106	0.720250
-0.139869	-0.507889	4.211213	0.000072	0.720542
-0.013266	-0.392068	4.221210	0.000048	0.720815
0.190301	-0.322700	4.231206	0.000010	0.721023
0.315105	-0.233795	4.241203	-0.000013	0.721242
-0.004186	-0.037459	4.251200	0.000046	0.721516
-0.005687	0.106606	4.261197	0.000046	0.721799
0.000000	0.307708	4.271194	0.000045	0.722197

0.223119	0.903985	4.276198	0.000003	0.723445
0.414882	2.127101	4.281203	-0.000034	0.725907
0.677933	3.931524	4.286208	-0.000084	0.729517
0.779911	6.320720	4.291213	-0.000105	0.734184
1.164579	9.157869	4.296218	-0.000178	0.739778
1.686391	12.466818	4.301222	-0.000278	0.746274
2.143049	16.241387	4.306227	-0.000365	0.753569
2.645055	20.409385	4.311232	-0.000461	0.761542
2.886796	25.031329	4.316237	-0.000509	0.770185
3.346408	29.970658	4.321242	-0.000598	0.779379
3.932089	35.245265	4.326246	-0.000711	0.789109
4.410188	40.856240	4.331251	-0.000804	0.799284
4.778559	46.788189	4.336256	-0.000876	0.809859
5.282225	52.982565	4.341261	-0.000974	0.820793
5.908177	59.421832	4.346266	-0.001095	0.832038
6.440889	66.108116	4.351270	-0.001198	0.843519
7.087078	72.997733	4.356275	-0.001323	0.855217
8.334978	79.983521	4.361280	-0.001560	0.867088
13.052382	86.606310	4.366285	-0.002443	0.879196
13.534604	94.177494	4.371290	-0.002538	0.891462
14.201710	101.872377	4.376294	-0.002667	0.903807
15.193667	109.660511	4.381299	-0.002857	0.916217
16.180446	117.558278	4.386304	-0.003046	0.928627
16.908804	125.631202	4.391309	-0.003187	0.941068
17.664212	133.788953	4.396314	-0.003333	0.953480
18.865924	141.960273	4.401318	-0.003562	0.965866
19.832052	150.250164	4.406323	-0.003747	0.978208
20.919693	158.601135	4.411328	-0.003955	0.990512
22.078724	166.996472	4.416333	-0.004176	1.002745
22.989674	175.473495	4.421338	-0.004352	1.014884
23.622059	184.034580	4.426342	-0.004475	1.026928
24.477915	192.602171	4.431347	-0.004640	1.038894
24.949143	201.241078	4.436352	-0.004733	1.050730
25.713163	209.863292	4.441357	-0.004881	1.062478
26.420463	218.514755	4.446362	-0.005019	1.074124
27.426221	227.107990	4.451366	-0.005212	1.085635
28.077526	235.785678	4.456371	-0.005339	1.097055
28.712485	244.454970	4.461376	-0.005463	1.108343
29.692214	253.084071	4.466381	-0.005651	1.119541
30.320051	261.760081	4.471386	-0.005773	1.130610
30.836503	270.456283	4.476390	-0.005875	1.141574
31.617844	279.120472	4.481395	-0.006026	1.152449
32.250168	287.761523	4.486400	-0.006150	1.163162
32.673024	296.439764	4.491405	-0.006234	1.173779
33.463243	305.020653	4.496410	-0.006387	1.184260
34.214991	313.624417	4.501414	-0.006533	1.194667
34.736768	322.232766	4.506419	-0.006635	1.204943
34.923823	330.889399	4.511424	-0.006676	1.215122
35.523449	339.457012	4.516429	-0.006793	1.225195
36.569792	347.961538	4.521434	-0.006994	1.235200
37.176338	356.501238	4.526438	-0.007112	1.245078
37.874439	365.032669	4.531443	-0.007248	1.254888
38.495065	373.536386	4.536448	-0.007369	1.264574
38.997427	382.080695	4.541453	-0.007468	1.274210
39.308013	390.606458	4.546458	-0.007531	1.283717
39.935589	399.090127	4.551462	-0.007654	1.293167
40.506785	407.559175	4.556467	-0.007766	1.302521
41.013109	416.105642	4.561472	-0.007866	1.311881
41.638245	424.572369	4.566477	-0.007988	1.321109
42.320606	432.961248	4.571482	-0.008120	1.330201
42.940473	441.369327	4.576486	-0.008241	1.339239
43.514900	449.779720	4.581491	-0.008354	1.348212
44.007543	458.189199	4.586496	-0.008451	1.357109
44.775094	466.527735	4.591501	-0.008599	1.365923
45.300017	474.913604	4.596506	-0.008703	1.374686
45.569795	483.325570	4.601510	-0.008758	1.383377
46.050333	491.712755	4.606515	-0.008853	1.392025
46.667065	500.035777	4.611520	-0.008974	1.400576
47.376028	508.353495	4.616525	-0.009111	1.409085
47.995796	516.680202	4.621530	-0.009232	1.417538
48.302290	525.037047	4.626534	-0.009294	1.425918
49.160749	533.335366	4.631539	-0.009460	1.434281
49.774955	541.631777	4.636544	-0.009580	1.442554
50.201224	549.973778	4.641549	-0.009664	1.450795
50.516279	558.320270	4.646554	-0.009729	1.458974
51.415234	566.549646	4.651558	-0.009901	1.467088
52.021944	574.900068	4.656563	-0.010020	1.475227
52.158903	583.223221	4.661568	-0.010051	1.483222
52.756967	591.489570	4.666573	-0.010168	1.491191
53.296215	599.753453	4.671578	-0.010273	1.499106
53.763364	608.017919	4.676582	-0.010366	1.506969
54.485394	616.273370	4.681587	-0.010506	1.514821
54.814525	624.542767	4.686592	-0.010572	1.522586
55.416457	632.795381	4.691597	-0.010690	1.530337
55.981886	641.046417	4.696602	-0.010801	1.538042
56.491440	649.294830	4.701606	-0.010901	1.545697
57.224222	657.542544	4.706611	-0.011043	1.553347
57.682973	665.770045	4.711616	-0.011134	1.560901
58.002811	674.040045	4.716621	-0.011199	1.568436
58.554788	682.259184	4.721626	-0.011307	1.575923
58.945087	690.493561	4.726630	-0.011385	1.583364
59.629424	698.700632	4.731635	-0.011518	1.590789
60.037006	706.937285	4.736640	-0.011599	1.598165
60.443289	715.160544	4.741645	-0.011680	1.605496
60.633694	723.428948	4.746650	-0.011721	1.612802
61.073019	731.632814	4.751654	-0.011808	1.620054
61.528417	739.853489	4.756659	-0.011898	1.627290
61.817052	748.125508	4.761664	-0.011958	1.634515
62.312853	756.296020	4.766669	-0.012055	1.641649
62.622718	764.491755	4.771674	-0.012118	1.648749
62.980068	772.693031	4.776678	-0.012190	1.655829
63.609542	780.854204	4.781683	-0.012313	1.662881
64.029550	789.031526	4.786688	-0.012396	1.669889
64.430693	797.237631	4.791693	-0.012476	1.676889
64.705544	805.414609	4.796698	-0.012533	1.683819
64.993948	813.611543	4.801702	-0.012592	1.690739
65.367226	821.809186	4.806707	-0.012667	1.697642
65.994566	829.930906	4.811712	-0.012789	1.704488
66.622415	838.105504	4.816717	-0.012911	1.711349
66.765904	846.322519	4.821722	-0.012944	1.718155
67.286742	854.464593	4.826726	-0.013046	1.724922
67.607089	862.659575	4.831731	-0.013111	1.731679
67.929279	870.837025	4.836736	-0.013176	1.738396
68.265383	879.000440	4.841741	-0.013244	1.745077
68.810446	887.152263	4.846746	-0.013351	1.751750
69.185387	895.320234	4.851750	-0.013426	1.758388
69.557598	903.470694	4.856755	-0.013501	1.764988
69.901575	911.630487	4.861760	-0.013570	1.771566
70.621927	919.753487	4.866765	-0.013710	1.778137
71.384183	927.835665	4.871770	-0.013857	1.784657
72.074198	935.992141	4.876774	-0.013991	1.791203
72.311726	944.224429	4.881779	-0.014040	1.797729
72.594008	952.357276	4.886784	-0.014098	1.804159
73.135975	960.486134	4.891789	-0.014205	1.810594
73.499122	968.653606	4.896794	-0.014278	1.817014
73.910125	976.781875	4.901798	-0.014360	1.823388
74.587871	984.909276	4.906803	-0.014491	1.829770
74.767970	993.093374	4.911808	-0.014530	1.836114
75.188401	1001.228497	4.916813	-0.014614	1.842427
75.702614	1009.339468	4.921818	-0.014715	1.848711
75.952139	1017.516173	4.926822	-0.014767	1.854993
76.132079	1025.678552	4.931827	-0.014805	1.861234
76.666232	1033.777421	4.936832	-0.014910	1.867448
77.117765	1041.944872	4.941837	-0.015000	1.873683
77.562546	1050.039243	4.946842	-0.015088	1.879841
77.831989	1058.170810	4.951846	-0.015143	1.885987
78.276156	1066.307656	4.956851	-0.015231	1.892137
78.509535	1074.448943	4.961856	-0.015280	1.898246
78.821967	1082.579321	4.966861	-0.015344	1.904336
79.403270	1090.680426	4.971866	-0.015457	1.910415
79.771227	1098.815156	4.976870	-0.015531	1.916476
80.201386	1106.925488	4.981875	-0.015616	1.922507
80.552342	1115.044699	4.986880	-0.015687	1.928516
81.135279	1123.156169	4.991885	-0.015801	1.934526
81.402966	1131.289613	4.996890	-0.015856	1.940499
81.446082	1139.454805	5.001894	-0.015870	1.946452
81.857066	1147.605449	5.006899	-0.015951	1.952417
82.194588	1155.711847	5.011904	-0.016020	1.958323
82.608751	1163.792814	5.016909	-0.016102	1.964201
83.072742	1171.873768	5.021914	-0.016194	1.970067
83.564657	1179.969179	5.026918	-0.016291	1.975929
83.971438	1188.072454	5.031923	-0.016372	1.981770
84.300288	1196.160298	5.036928	-0.016438	1.987574
84.823318	1204.288101	5.041933	-0.016541	1.993410
85.276314	1212.374290	5.046938	-0.016631	1.999192
85.533552	1220.480541	5.051942	-0.016684	2.004951
86.138114	1228.581166	5.056947	-0.016802	2.010726
86.756748	1236.669724	5.061952	-0.016922	2.016477
87.091585	1244.796533	5.066957	-0.016990	2.022208
87.674619	1252.872812	5.071962	-0.017104	2.027914
88.092028	1261.027404	5.076966	-0.017187	2.033641
88.488954	1269.133915	5.081971	-0.017266	2.039317
88.760454	1277.210931	5.086976	-0.017322	2.044943
89.465499	1285.279965	5.091981	-0.017459	2.050593
89.793274	1293.409315	5.096986	-0.017525	2.056230
90.168055	1301.499138	5.101990	-0.017600	2.061829
90.663224	1309.594854	5.106995	-0.017698	2.067429
91.057067	1317.708485	5.112000	-0.017776	2.073016
91.172249	1325.848869	5.117005	-0.017803	2.078578
91.413818	1333.944317	5.122010	-0.017853	2.084107
91.897235	1342.014414	5.127014	-0.017949	2.089629
92.307949	1350.139426	5.132019	-0.018031	2.095165
92.639670	1358.224716	5.137024	-0.018098	2.100653
93.239401	1366.300379	5.142029	-0.018215	2.106145
93.443128	1374.451695	5.147034	-0.018258	2.111636
93.804972	1382.570107	5.152038	-0.018331	2.117105
94.098378	1390.653403	5.157043	-0.018391	2.122530
94.573455	1398.696090	5.162048	-0.018484	2.127932
94.987743	1406.801252	5.167053	-0.018567	2.133356
95.170954	1414.889469	5.172058	-0.018606	2.138732
95.887428	1422.910091	5.177062	-0.018745	2.144101
96.488700	1430.983240	5.182067	-0.018862	2.149480
96.571890	1439.121038	5.187072	-0.018883	2.154839
97.042640	1447.183462	5.192077	-0.018976	2.160172
97.444748	1455.258028	5.197082	-0.019056	2.165493
97.607048	1463.379652	5.202086	-0.019092	2.170809
97.987138	1471.477947	5.207091	-0.019168	2.176117
98.392059	1479.519649	5.212096	-0.019248	2.181378
98.810331	1487.611028	5.217101	-0.019332	2.186659
99.022939	1495.749412	5.222106	-0.019377	2.191939
99.416535	1503.830438	5.227110	-0.019455	2.197186
99.986653	1511.874880	5.232115	-0.019567	2.202413
99.990777	1519.980733	5.237120	-0.019573	2.207615
100.600142	1528.047071	5.242125	-0.019691	2.212835
100.853305	1536.127580	5.247130	-0.019744	2.218019
101.100552	1544.208156	5.252134	-0.019795	2.223190
101.497241	1552.287083	5.257139	-0.019874	2.228362
101.880981	1560.375555	5.262144	-0.019951	2.233526
102.403033	1568.410156	5.267149	-0.020054	2.238657
102.640894	1576.496723	5.272154	-0.020103	2.243783
103.131580	1584.548197	5.277158	-0.020200	2.248898
103.693695	1592.637540	5.282163	-0.020310	2.254031
104.119224	1600.691406	5.287168	-0.020394	2.259118
104.907545	1608.730986	5.292173	-0.020547	2.264216
105.465232	1616.820402	5.297178	-0.020656	2.269314
105.662339	1625.019862	5.302182	-0.020698	2.274437
106.040168	1633.060642	5.307187	-0.020773	2.279466
106.183799	1641.136329	5.312192	-0.020806	2.284486
106.586388	1649.213483	5.317197	-0.020886	2.289517
106.740509	1657.314206	5.322202	-0.020920	2.294531
106.968185	1665.357988	5.327206	-0.020967	2.299504
107.381239	1673.428048	5.332211	-0.021050	2.304499
107.573469	1681.505333	5.337216	-0.021091	2.309469
108.019936	1689.578225	5.342221	-0.021179	2.314447
108.398464	1697.613845	5.347226	-0.021255	2.319385
108.814920	1705.657084	5.352230	-0.021338	2.324320
109.134909	1713.740852	5.357235	-0.021403	2.329262
109.255823	1721.847401	5.362240	-0.021431	2.334191
109.682946	1729.908003	5.367245	-0.021515	2.339106
110.044996	1737.969582	5.372250	-0.021588	2.344006
110.431383	1746.022192	5.377254	-0.021665	2.348893
111.391555	1754.070269	5.382259	-0.021849	2.353813
111.454165	1762.146680	5.387264	-0.021866	2.358667
111.844700	1770.207925	5.392269	-0.021944	2.363529
112.637556	1778.228080	5.397274	-0.022097	2.368388
112.635455	1786.370306	5.402278	-0.022102	2.373246
113.280905	1794.411534	5.407283	-0.022228	2.378086
113.559311	1802.465293	5.412288	-0.022285	2.382894
114.069895	1810.524273	5.417293	-0.022385	2.387713
114.419035	1818.623527	5.422298	-0.022456	2.392534
114.802364	1826.670258	5.427302	-0.022532	2.397317
115.203614	1834.731471	5.432307	-0.022612	2.402100
115.319043	1842.814565	5.437312	-0.022639	2.406865
115.509695	1850.917897	5.442317	-0.022680	2.411637
116.028081	1858.959375	5.447322	-0.022782	2.416389
116.335942	1867.014663	5.452326	-0.022844	2.421124
116.665581	1875.086806	5.457331	-0.022911	2.425860
116.904527	1883.179391	5.462336	-0.022961	2.430593
117.375336	1891.299878	5.467341	-0.023054	2.435350
117.755253	1899.318701	5.472346	-0.023130	2.440032
117.957394	1907.350328	5.477350	-0.023173	2.444698
118.447244	1915.405177	5.482355	-0.023269	2.449391
118.511397	1923.493550	5.487360	-0.023286	2.454062
118.899542	1931.545312	5.492365	-0.023364	2.458727
119.199308	1939.596691	5.497370	-0.023425	2.463377
119.531834	1947.648324	5.502374	-0.023492	2.468020
119.998363	1955.715665	5.507379	-0.023585	2.472674
120.286503	1963.757684	5.512384	-0.023643	2.477291
120.686137	1971.786754	5.517389	-0.023723	2.481900
121.075215	1979.845280	5.522394	-0.023801	2.486516
121.206645	1987.922629	5.527398	-0.023831	2.491116
121.765176	1995.972855	5.532403	-0.023940	2.495723
122.029199	2004.041755	5.537408	-0.023994	2.500311
122.278823	2012.077735	5.542413	-0.024046	2.504870
122.580540	2020.159228	5.547418	-0.024108	2.509450
122.838329	2028.280190	5.552422	-0.024161	2.514041
123.333587	2036.294308	5.557427	-0.024259	2.518581
123.923602	2044.286587	5.562432	-0.024374	2.523107
124.226025	2052.349825	5.567437	-0.024435	2.527644
124.362718	2060.442714	5.572442	-0.024466	2.532177
124.592080	2068.508172	5.577446	-0.024514	2.536694
125.204965	2076.541688	5.582451	-0.024633	2.541212
125.264192	2084.592942	5.587456	-0.024650	2.545692
125.658672	2092.661300	5.592461	-0.024728	2.550198
126.043804	2100.735493	5.597466	-0.024806	2.554698
126.516568	2108.739092	5.602470	-0.024899	2.559158
126.992859	2116.771506	5.607475	-0.024993	2.563625
127.196160	2124.838693	5.612480	-0.025036	2.568085
127.751355	2132.887757	5.617485	-0.025145	2.572552
127.953684	2140.989447	5.622490	-0.025188	2.577015
128.083804	2149.040549	5.627494	-0.025217	2.581438
128.707780	2157.068061	5.632499	-0.025339	2.585874
128.919002	2165.154985	5.637504	-0.025383	2.590306
129.197979	2173.405010	5.642509	-0.025441	2.594825
129.546558	2181.380002	5.647514	-0.025511	2.599190
129.670246	2189.371269	5.652518	-0.025539	2.603542
130.109244	2197.392731	5.657523	-0.025626	2.607925
130.248002	2205.449571	5.662528	-0.025657	2.612298
130.771815	2213.482792	5.667533	-0.025760	2.616678
131.124700	2221.511253	5.672538	-0.025831	2.621036
131.335996	2229.558286	5.677542	-0.025876	2.625387
131.752499	2237.614455	5.682547	-0.025958	2.629750
132.311951	2245.641105	5.687552	-0.026068	2.634098
132.865389	2253.645687	5.692557	-0.026176	2.638428
133.222687	2261.697114	5.697562	-0.026248	2.642762
133.376185	2269.752997	5.702566	-0.026282	2.647078
133.865638	2277.812440	5.707571	-0.026378	2.651411
134.295443	2285.863021	5.712576	-0.026464	2.655728
134.675235	2293.906030	5.717581	-0.026540	2.660031
134.978326	2301.969259	5.722586	-0.026601	2.664332
135.154923	2310.027459	5.727590	-0.026640	2.668616
135.571675	2318.120993	5.732595	-0.026722	2.672927
135.769012	2326.170418	5.737600	-0.026765	2.677193
136.178004	2334.182984	5.742605	-0.026846	2.681447
136.516546	2342.218790	5.747610	-0.026914	2.685702
136.670567	2350.271327	5.752614	-0.026948	2.689947
136.963560	2358.345578	5.757619	-0.027008	2.694205
137.201850	2366.389878	5.762624	-0.027058	2.698438
137.701841	2374.398915	5.767629	-0.027156	2.702661
137.993240	2382.472014	5.772634	-0.027216	2.706899
138.062623	2390.525753	5.777638	-0.027234	2.711106
138.336040	2398.612723	5.782643	-0.027290	2.715336
138.741503	2406.600667	5.787648	-0.027371	2.719517
138.960425	2414.635924	5.792653	-0.027417	2.723703
139.182065	2422.688178	5.797658	-0.027463	2.727893
139.787066	2430.702755	5.802662	-0.027581	2.732080
140.249984	2438.790888	5.807667	-0.027673	2.736290
140.277404	2446.835371	5.812672	-0.027683	2.740444
140.523471	2454.877253	5.817677	-0.027734	2.744603
140.842104	2462.964847	5.822682	-0.027799	2.748785
141.148526	2471.038410	5.827686	-0.027861	2.752952
141.132429	2479.135375	5.832691	-0.027864	2.757105
141.232832	2487.136392	5.837696	-0.027888	2.761210
141.653994	2495.133918	5.842701	-0.027971	2.765326
141.841585	2503.187347	5.847706	-0.028012	2.769450
142.211122	2511.207220	5.852710	-0.028086	2.773562
142.438885	2519.269180	5.857715	-0.028133	2.777681
142.738506	2527.272236	5.862720	-0.028194	2.781768
143.116196	2535.316968	5.867725	-0.028270	2.785875
143.434442	2543.384361	5.872730	-0.028335	2.789983
143.357986	2551.477278	5.877734	-0.028326	2.794076
143.787205	2559.500295	5.882739	-0.028411	2.798156
144.168630	2567.503629	5.887744	-0.028487	2.802218
144.432322	2575.547188	5.892749	-0.028542	2.806287
144.649491	2583.593009	5.897754	-0.028587	2.810349
144.860327	2591.651947	5.902758	-0.028632	2.814411
145.273430	2599.672784	5.907763	-0.028714	2.818459
145.355026	2607.710137	5.912768	-0.028734	2.822491
145.717487	2615.734567	5.917773	-0.028807	2.826527
146.141081	2623.789368	5.922778	-0.028891	2.830576
146.344271	2631.880941	5.927782	-0.028935	2.834624
146.572509	2639.923048	5.932787	-0.028982	2.838644
146.725637	2647.927404	5.937792	-0.029016	2.842635
147.051187	2655.947545	5.942797	-0.029082	2.846638
147.042272	2664.036351	5.947802	-0.029086	2.850650
147.444757	2672.044271	5.952806	-0.029166	2.854640
147.802932	2680.088172	5.957811	-0.029238	2.858639
147.911660	2688.117102	5.962816	-0.029263	2.862611
148.005902	2696.182936	5.967821	-0.029286	2.866596
148.338856	2704.235940	5.972826	-0.029354	2.870581
148.751850	2712.265371	5.977830	-0.029436	2.874554
148.954734	2720.324429	5.982835	-0.029479	2.878524
149.325321	2728.328985	5.987840	-0.029553	2.882471
149.707892	2736.349134	5.992845	-0.029630	2.886421
149.975767	2744.395093	5.997850	-0.029685	2.890372
150.253956	2752.454912	6.002854	-0.029742	2.894325
150.652679	2760.489567	6.007859	-0.029821	2.898267
150.760977	2768.544265	6.012864	-0.029847	2.902197
150.830244	2776.589838	6.017869	-0.029865	2.906115
151.017167	2784.628268	6.022874	-0.029905	2.910031
151.133765	2792.766454	6.027878	-0.029932	2.913986
151.469088	2800.771312	6.032883	-0.030000	2.917883
151.527074	2808.757919	6.037888	-0.030016	2.921751
152.019790	2816.764699	6.042893	-0.030113	2.925647
152.129255	2824.804012	6.047898	-0.030139	2.929533
152.278988	2832.865252	6.052902	-0.030172	2.933427
152.624921	2840.892680	6.057907	-0.030241	2.937309
152.964705	2848.899093	6.062912	-0.030310	2.941175
152.972686	2856.943573	6.067917	-0.030317	2.945038
153.251942	2864.990260	6.072922	-0.030374	2.948910
153.485619	2873.053886	6.077926	-0.030423	2.952784
153.513511	2881.139208	6.082931	-0.030433	2.956651
153.811280	2889.110075	6.087936	-0.030494	2.960473
153.881459	2897.149800	6.092941	-0.030512	2.964312
154.121796	2905.196915	6.097946	-0.030562	2.968157
154.294965	2913.231548	6.102950	-0.030600	2.971988
154.625854	2921.279605	6.107955	-0.030667	2.975828
154.899232	2929.287722	6.112960	-0.030723	2.979642
155.088169	2937.327063	6.117965	-0.030763	2.983461
155.719443	2945.346545	6.122970	-0.030886	2.987288
155.491723	2953.423024	6.127974	-0.030849	2.991094
156.008100	2961.473650	6.132979	-0.030951	2.994920
156.358973	2969.455507	6.137984	-0.031021	2.998700
156.516764	2977.516326	6.142989	-0.031056	3.002504
156.780605	2985.532502	6.147994	-0.031110	3.006286
156.916891	2993.550970	6.152998	-0.031141	3.010059
157.081182	3001.651914	6.158003	-0.031177	3.013867
157.340138	3009.663979	6.163008	-0.031230	3.017633
157.530356	3017.696681	6.168013	-0.031271	3.021400
157.808733	3025.706301	6.173018	-0.031328	3.025157
158.066831	3033.742856	6.178022	-0.031381	3.028920
158.224358	3041.830103	6.183027	-0.031416	3.032697
158.353801	3049.872712	6.188032	-0.031445	3.036448
158.772892	3057.847810	6.193037	-0.031529	3.040176
158.926769	3065.874309	6.198042	-0.031563	3.043911
159.154483	3073.905199	6.203046	-0.031610	3.047647
159.531889	3081.971202	6.208051	-0.031686	3.051401
159.765558	3090.007343	6.213056	-0.031735	3.055131
159.922473	3098.037600	6.218061	-0.031769	3.058849
160.172563	3106.086506	6.223066	-0.031821	3.062576
160.570188	3114.086994	6.228070	-0.031900	3.066282
160.937601	3122.118757	6.233075	-0.031974	3.069998
161.095360	3130.259787	6.238080	-0.032009	3.073749
161.319919	3138.263995	6.243085	-0.032056	3.077435
161.566677	3146.287942	6.248090	-0.032107	3.081128
161.685690	3154.267689	6.253094	-0.032134	3.084790
162.016686	3162.299860	6.258099	-0.032201	3.088481
162.100208	3170.367305	6.263104	-0.032222	3.092172
162.290575	3178.420752	6.268109	-0.032263	3.095858
162.595834	3186.414888	6.273114	-0.032325	3.099517
162.736806	3194.456950	6.278118	-0.032357	3.103186
162.795722	3202.533250	6.283123	-0.032373	3.106863
162.807002	3210.548258	6.288128	-0.032380	3.110506
163.294606	3218.555781	6.293133	-0.032476	3.114162
163.753745	3226.567516	6.298138	-0.032567	3.117814
163.656623	3234.621684	6.303142	-0.032554	3.121457
164.049148	3242.612144	6.308147	-0.032633	3.125088
164.239316	3250.666564	6.313152	-0.032673	3.128735
164.370109	3258.727307	6.318157	-0.032703	3.132377
164.652294	3266.794476	6.323162	-0.032761	3.136025
164.899022	3274.774720	6.328166	-0.032812	3.139629
165.133999	3282.811264	6.333171	-0.032861	3.143252
165.155416	3290.852941	6.338176	-0.032870	3.146865
165.432939	3298.889460	6.343181	-0.032927	3.150482
165.716909	3306.959140	6.348186	-0.032985	3.154110
166.005627	3314.944971	6.353190	-0.033044	3.157697
166.056006	3323.012644	6.358195	-0.033059	3.161305
166.441436	3330.971957	6.363200	-0.033136	3.164876
166.551757	3339.039734	6.368205	-0.033162	3.168479
166.814509	3347.093726	6.373210	-0.033216	3.172078
166.988202	3355.105860	6.378214	-0.033254	3.175651
167.446056	3363.121758	6.383219	-0.033344	3.179234
167.446506	3371.195455	6.388224	-0.033350	3.182818
167.822559	3379.206614	6.393229	-0.033425	3.186387
168.227570	3387.252408	6.398234	-0.033506	3.189968
168.266794	3395.281388	6.403238	-0.033518	3.193523
168.648233	3403.321623	6.408243	-0.033595	3.197092
168.921031	3411.331056	6.413248	-0.033651	3.200640
168.994822	3419.322917	6.418253	-0.033670	3.204168
169.093662	3427.396441	6.423258	-0.033693	3.207728
169.402847	3435.428750	6.428262	-0.033756	3.211275
169.731747	3443.457596	6.433267	-0.033823	3.214818
169.860925	3451.485653	6.438272	-0.033852	3.218348
169.993192	3459.525869	6.443277	-0.033882	3.221880
170.499915	3467.516644	6.448282	-0.033982	3.225401
170.717298	3475.542533	6.453286	-0.034027	3.228922
171.127388	3483.634495	6.458291	-0.034109	3.232476
171.234928	3491.703422	6.463296	-0.034134	3.236003
171.656138	3499.638433	6.468301	-0.034218	3.239481
171.848970	3507.676318	6.473306	-0.034259	3.242991
172.131559	3515.695397	6.478310	-0.034317	3.246492
172.643024	3523.685794	6.483315	-0.034418	3.249986
172.563086	3531.793036	6.488320	-0.034408	3.253504
172.574392	3539.819333	6.493325	-0.034415	3.256986
172.967573	3547.809396	6.498330	-0.034494	3.260464
173.151618	3555.843052	6.503334	-0.034533	3.263949
173.281849	3563.918440	6.508339	-0.034563	3.267446
173.594830	3571.933239	6.513344	-0.034626	3.270920
174.044767	3579.946540	6.518349	-0.034716	3.274395
174.228487	3587.998337	6.523354	-0.034755	3.277873
174.341303	3596.019444	6.528358	-0.034781	3.281331
174.768012	3603.999885	6.533363	-0.034866	3.284780
174.947544	3612.065556	6.538368	-0.034905	3.288252
175.168523	3620.115772	6.543373	-0.034951	3.291715
175.425201	3628.138618	6.548378	-0.035004	3.295165
175.453617	3636.164020	6.553382	-0.035015	3.298603
176.024632	3644.173094	6.558387	-0.035126	3.302051
176.247466	3652.190916	6.563392	-0.035173	3.305487
176.616480	3660.210881	6.568397	-0.035247	3.308924
176.941593	3668.299634	6.573402	-0.035313	3.312386
177.064434	3676.342196	6.578406	-0.035341	3.315818
177.297316	3684.337274	6.583411	-0.035390	3.319229
177.227418	3692.371580	6.588416	-0.035382	3.322642
177.563846	3700.363963	6.593421	-0.035450	3.326049
177.933914	3708.393438	6.598426	-0.035524	3.329470
177.942906	3716.436922	6.603430	-0.035531	3.332879
178.176470	3724.506818	6.608435	-0.035580	3.336305
178.311533	3732.511673	6.613440	-0.035610	3.339696
178.515961	3740.515055	6.618445	-0.035654	3.343085
178.871370	3748.552149	6.623450	-0.035725	3.346490
179.107521	3756.582663	6.628454	-0.035774	3.349885
179.242866	3764.671605	6.633459	-0.035805	3.353297
179.365725	3772.701639	6.638464	-0.035833	3.356681
179.561980	3780.689743	6.643469	-0.035875	3.360046
179.815326	3788.702668	6.648474	-0.035927	3.363421
179.761755	3796.746844	6.653478	-0.035923	3.366794
180.263056	3804.755801	6.658483	-0.036021	3.370168
180.322041	3812.831295	6.663488	-0.036037	3.373551
180.385894	3820.851792	6.668493	-0.036055	3.376909
180.637727	3828.866741	6.673498	-0.036107	3.380267
180.803728	3836.857332	6.678502	-0.036143	3.383608
181.255179	3844.898673	6.683507	-0.036232	3.386977
181.589179	3852.918316	6.688512	-0.036300	3.390330
181.901589	3861.010155	6.693517	-0.036363	3.393709
182.248974	3869.034436	6.698522	-0.036433	3.397057
182.397132	3876.999102	6.703526	-0.036466	3.400370
182.764669	3884.988090	6.708531	-0.036540	3.403698
183.029862	3893.040994	6.713536	-0.036594	3.407046
183.146024	3901.045587	6.718541	-0.036621	3.410365
183.315689	3909.134425	6.723546	-0.036658	3.413717
183.516980	3917.147096	6.728550	-0.036701	3.417036
183.969563	3925.130475	6.733555	-0.036790	3.420347
184.084846	3933.180362	6.738560	-0.036817	3.423672
184.009309	3941.227890	6.743565	-0.036808	3.426986
184.595516	3949.222649	6.748570	-0.036923	3.430297
184.947124	3957.267950	6.753574	-0.036994	3.433618
185.283113	3965.288268	6.758579	-0.037061	3.436925
185.514037	3973.292984	6.763584	-0.037110	3.440219
185.812548	3981.302339	6.768589	-0.037170	3.443513
186.042141	3989.395174	6.773594	-0.037219	3.446837
186.160713	3997.385009	6.778598	-0.037246	3.450111
186.296500	4005.467434	6.783603	-0.037276	3.453421
186.719101	4013.495104	6.788608	-0.037360	3.456714
187.118682	4021.472005	6.793613	-0.037440	3.459983
187.428193	4029.501311	6.798618	-0.037503	3.463267
187.407491	4037.570606	6.803622	-0.037504	3.466553
187.576423	4045.588101	6.808627	-0.037541	3.469822
187.664640	4053.676433	6.813632	-0.037563	3.473113
188.041041	4061.655316	6.818637	-0.037638	3.476367
188.214254	4069.658514	6.823642	-0.037676	3.479620
188.202845	4077.651335	6.828646	-0.037679	3.482860
188.482634	4085.684463	6.833651	-0.037736	3.486123
188.645603	4093.728918	6.838656	-0.037772	3.489384
188.789832	4101.749984	6.843661	-0.037804	3.492631
189.018685	4109.818452	6.848666	-0.037852	3.495897
189.292443	4117.778118	6.853670	-0.037908	3.499118
189.356413	4125.828767	6.858675	-0.037925	3.502366
189.631713	4133.819554	6.863680	-0.037982	3.505593
189.830013	4141.848561	6.868685	-0.038024	3.508830
190.242592	4149.902929	6.873690	-0.038106	3.512081
190.304591	4157.925520	6.878694	-0.038123	3.515306
190.575888	4165.929521	6.883699	-0.038179	3.518526
190.982343	4173.978285	6.888704	-0.038260	3.521765
191.110604	4181.972990	6.893709	-0.038289	3.524972
191.445423	4190.028178	6.898714	-0.038357	3.528206
191.857836	4198.032755	6.903718	-0.038439	3.531418
191.998842	4206.113615	6.908723	-0.038470	3.534651
192.123905	4214.149915	6.913728	-0.038499	3.537862
192.372540	4222.142862	6.918733	-0.038550	3.541056
192.588826	4230.179266	6.923738	-0.038596	3.544264
192.452858	4238.227960	6.928742	-0.038576	3.547463
192.756362	4246.244329	6.933747	-0.038638	3.550660
193.124849	4254.362342	6.938752	-0.038712	3.553896
193.359351	4262.347477	6.943757	-0.038760	3.557072
193.755822	4270.284675	6.948762	-0.038839	3.560231
194.012977	4278.287381	6.953766	-0.038893	3.563410
194.361327	4286.327793	6.958771	-0.038963	3.566602
194.571031	4294.305892	6.963776	-0.039007	3.569764
194.829015	4302.378568	6.968781	-0.039060	3.572961
195.006958	4310.456475	6.973786	-0.039099	3.576155
195.144496	4318.420284	6.978790	-0.039130	3.579300
195.393595	4326.441794	6.983795	-0.039181	3.582468
195.636870	4334.465391	6.988800	-0.039232	3.585634
195.709822	4342.483765	6.993805	-0.039251	3.588791
195.785342	4350.554352	6.998810	-0.039270	3.591965
196.163030	4358.535862	7.003814	-0.039346	3.595110
196.608803	4366.560312	7.008819	-0.039434	3.598270
196.645358	4374.599457	7.013824	-0.039446	3.601423
196.808177	4382.563394	7.018829	-0.039482	3.604546
197.018310	4390.632363	7.023834	-0.039526	3.607710
197.003774	4398.665157	7.028838	-0.039529	3.610850
197.490412	4406.713067	7.033843	-0.039625	3.614007
197.785076	4414.717609	7.038848	-0.039685	3.617139
197.958868	4422.712805	7.043853	-0.039722	3.620261
198.002758	4430.767290	7.048858	-0.039736	3.623400
198.299597	4438.767964	7.053862	-0.039796	3.626522
198.721427	4446.795164	7.058867	-0.039880	3.629656
198.797356	4454.879809	7.063872	-0.039900	3.632799
198.913185	4462.889923	7.068877	-0.039926	3.635912
199.204222	4470.890150	7.073882	-0.039986	3.639023
199.463678	4478.909186	7.078886	-0.040039	3.642138
199.824789	4486.892811	7.083891	-0.040112	3.645239
199.757850	4494.964891	7.088896	-0.040105	3.648360
199.869423	4503.015636	7.093901	-0.040131	3.651476
200.115981	4511.048046	7.098906	-0.040182	3.654585
200.413293	4519.041108	7.103910	-0.040243	3.657677
200.615221	4527.070146	7.108915	-0.040285	3.660778
200.809131	4535.110679	7.113920	-0.040327	3.663881
200.939028	4543.098285	7.118925	-0.040356	3.666959
201.426528	4551.146882	7.123930	-0.040452	3.670067
201.443533	4559.184098	7.128934	-0.040461	3.673155
201.670035	4567.202063	7.133939	-0.040508	3.676240
201.869216	4575.200173	7.138944	-0.040551	3.679313
202.139222	4583.206123	7.143949	-0.040606	3.682388
202.214052	4591.238187	7.148954	-0.040625	3.685466
202.384597	4599.247909	7.153958	-0.040662	3.688536
202.789428	4607.277742	7.158963	-0.040743	3.691616
203.103297	4615.300745	7.163968	-0.040807	3.694689
203.094261	4623.348991	7.168973	-0.040810	3.697760
203.559018	4631.361118	7.173978	-0.040902	3.700827
203.767316	4639.344124	7.178982	-0.040946	3.703874
203.699304	4647.397439	7.183987	-0.040939	3.706939
203.890178	4655.414592	7.188992	-0.040980	3.709994
204.211679	4663.495044	7.193997	-0.041045	3.713073
204.585903	4671.568319	7.199002	-0.041120	3.716148
204.624320	4679.498502	7.204006	-0.041132	3.719158
205.127726	4687.523603	7.209011	-0.041231	3.722213
205.110408	4695.528082	7.214016	-0.041233	3.725245
205.571381	4703.505807	7.219021	-0.041324	3.728276
206.039559	4711.550892	7.224026	-0.041417	3.731330
205.941767	4719.620675	7.229030	-0.041404	3.734377
206.080387	4727.638499	7.234035	-0.041435	3.737408
206.312316	4735.628981	7.239040	-0.041483	3.740428
206.561242	4743.617526	7.244045	-0.041535	3.743446
206.851185	4751.694685	7.249050	-0.041594	3.746495
206.970512	4759.696907	7.254054	-0.041622	3.749510
207.288119	4767.755803	7.259059	-0.041686	3.752548
207.348981	4775.822883	7.264064	-0.041703	3.755580
207.406307	4783.814380	7.269069	-0.041719	3.758582
207.695740	4791.831554	7.274074	-0.041778	3.761596
207.844050	4799.812981	7.279078	-0.041811	3.764592
208.116621	4807.860909	7.284083	-0.041867	3.767612
208.358368	4815.879716	7.289088	-0.041917	3.770619
208.579731	4823.906255	7.294093	-0.041964	3.773625
208.873486	4831.968426	7.299098	-0.042024	3.776644
209.033214	4839.924673	7.304102	-0.042059	3.779618
209.403246	4847.956875	7.309107	-0.042133	3.782623
209.613878	4855.999163	7.314112	-0.042177	3.785625
209.578691	4864.022962	7.319117	-0.042176	3.788613
209.803212	4872.094111	7.324122	-0.042223	3.791622
210.166734	4880.114955	7.329126	-0.042296	3.794612
210.543851	4888.080141	7.334131	-0.042371	3.797580
210.686851	4896.096423	7.339136	-0.042403	3.800559
210.920967	4904.042242	7.344141	-0.042452	3.803512
211.144193	4912.139047	7.349146	-0.042499	3.806518
211.323745	4920.116695	7.354150	-0.042538	3.809477
211.733922	4928.176054	7.359155	-0.042619	3.812469
212.111426	4936.188052	7.364160	-0.042695	3.815439
212.151141	4944.192680	7.369165	-0.042708	3.818398
212.304944	4952.243610	7.374170	-0.042742	3.821374
212.426712	4960.259523	7.379174	-0.042769	3.824334
212.648976	4968.253187	7.384179	-0.042816	3.827286
213.105904	4976.312903	7.389184	-0.042907	3.830264
213.189575	4984.315071	7.394189	-0.042927	3.833211
213.494329	4992.393521	7.399194	-0.042989	3.836189
213.459113	5000.365497	7.404198	-0.042988	3.839118
213.786559	5008.375412	7.409203	-0.043054	3.842066
214.036697	5016.399287	7.414208	-0.043106	3.845015
214.030720	5024.393219	7.419213	-0.043110	3.847946
214.449814	5032.461251	7.424218	-0.043194	3.850910
214.722631	5040.465161	7.429222	-0.043250	3.853846
214.974196	5048.567807	7.434227	-0.043302	3.856815
215.008142	5056.555277	7.439232	-0.043313	3.859735
215.105154	5064.533453	7.444237	-0.043337	3.862651
215.288265	5072.605508	7.449242	-0.043376	3.865601
215.527960	5080.589159	7.454246	-0.043426	3.868517
215.700046	5088.645108	7.459251	-0.043463	3.871456
215.988812	5096.957530	7.464256	-0.043523	3.874489
216.129177	5104.839799	7.469261	-0.043554	3.877359
216.380083	5112.756517	7.474266	-0.043606	3.880243
216.528800	5120.730159	7.479270	-0.043639	3.883142
216.759848	5128.714133	7.484275	-0.043687	3.886045
216.980565	5136.760684	7.489280	-0.043733	3.888968
217.282062	5144.781632	7.494285	-0.043795	3.891881
217.794178	5152.821990	7.499290	-0.043895	3.894803
217.878447	5160.818148	7.504294	-0.043916	3.897699
218.164805	5168.755531	7.509299	-0.043975	3.900575
218.364277	5176.839019	7.514304	-0.044017	3.903500
218.233608	5184.852055	7.519309	-0.043998	3.906391
218.622189	5192.880150	7.524314	-0.044076	3.909295
218.889396	5200.907525	7.529318	-0.044131	3.912195
219.055946	5208.943438	7.534323	-0.044167	3.915093
219.302598	5216.975301	7.539328	-0.044219	3.917989
219.598129	5224.911821	7.544333	-0.044279	3.920850
219.634852	5232.959216	7.549338	-0.044291	3.923744
219.603792	5241.023755	7.554342	-0.044290	3.926641
219.786123	5249.019341	7.559347	-0.044330	3.929514
220.178914	5257.034909	7.564352	-0.044408	3.932396
220.219693	5265.053711	7.569357	-0.044421	3.935271
220.365239	5273.087248	7.574362	-0.044453	3.938151
220.503018	5281.094828	7.579366	-0.044484	3.941020
220.723378	5289.085981	7.584371	-0.044530	3.943882
220.945570	5297.130139	7.589376	-0.044577	3.946761
221.301862	5305.102138	7.594381	-0.044649	3.949614
221.522082	5313.193322	7.599386	-0.044695	3.952505
221.662543	5321.227765	7.604390	-0.044726	3.955373
221.689562	5329.248059	7.609395	-0.044737	3.958231
222.014980	5337.246071	7.614400	-0.044803	3.961085
221.999917	5345.238771	7.619405	-0.044805	3.963928
222.383448	5353.250197	7.624410	-0.044882	3.966784
222.599853	5361.241067	7.629414	-0.044927	3.969626
222.718418	5369.288919	7.634419	-0.044955	3.972486
222.877749	5377.366273	7.639424	-0.044990	3.975354
222.959323	5385.361499	7.644429	-0.045010	3.978190
223.170324	5393.406796	7.649434	-0.045055	3.981044
223.326789	5401.359883	7.654438	-0.045089	3.983862
223.454332	5409.410031	7.659443	-0.045118	3.986713
223.898448	5417.447282	7.664448	-0.045206	3.989561
224.160111	5425.464203	7.669453	-0.045260	3.992397
224.285876	5433.528417	7.674458	-0.045289	3.995246
224.307543	5441.550856	7.679462	-0.045298	3.998077
224.446725	5449.509105	7.684467	-0.045329	4.000884
224.821295	5457.521122	7.689472	-0.045404	4.003712
225.035024	5465.550483	7.694477	-0.045449	4.006542
225.341962	5473.588639	7.699482	-0.045512	4.009375
225.524731	5481.638919	7.704486	-0.045551	4.012207
225.469711	5489.662618	7.709491	-0.045546	4.015025
225.782077	5497.707203	7.714496	-0.045610	4.017853
226.098111	5505.654157	7.719501	-0.045674	4.020646
226.251603	5513.708181	7.724506	-0.045707	4.023471
226.421972	5521.693214	7.729510	-0.045744	4.026271
226.627302	5529.727013	7.734515	-0.045788	4.029086
226.820424	5537.798292	7.739520	-0.045829	4.031912
227.092046	5545.904190	7.744525	-0.045885	4.034749
227.520429	5553.877921	7.749530	-0.045970	4.037540
227.763601	5561.811383	7.754534	-0.046021	4.040313
227.794068	5569.827268	7.759539	-0.046032	4.043109
228.073890	5577.813349	7.764544	-0.046089	4.045897
228.231115	5585.826235	7.769549	-0.046123	4.048690
228.628641	5593.873494	7.774554	-0.046203	4.051497
228.862271	5601.913418	7.779558	-0.046252	4.054297
228.952087	5609.941463	7.784563	-0.046274	4.057088
229.411984	5617.916126	7.789568	-0.046364	4.059865
229.450295	5625.921436	7.794573	-0.046377	4.062644
229.558935	5633.923144	7.799578	-0.046402	4.065421
229.710872	5641.964699	7.804582	-0.046436	4.068211
229.933264	5649.966688	7.809587	-0.046483	4.070985
230.389237	5658.044459	7.814592	-0.046573	4.073788
230.293375	5666.052952	7.819597	-0.046560	4.076557
230.499016	5674.050616	7.824602	-0.046604	4.079324
230.674978	5682.099253	7.829606	-0.046642	4.082107
230.888643	5690.019923	7.834611	-0.046687	4.084844
231.269966	5698.070855	7.839616	-0.046763	4.087626
231.257539	5706.096236	7.844621	-0.046766	4.090392
231.580896	5714.174161	7.849626	-0.046832	4.093179
231.649406	5722.196582	7.854630	-0.046850	4.095942
231.998411	5730.192147	7.859635	-0.046920	4.098697
232.357926	5738.193762	7.864640	-0.046992	4.101453
232.470323	5746.170089	7.869645	-0.047018	4.104194
232.590438	5754.268865	7.874650	-0.047046	4.106976
232.675969	5762.286164	7.879654	-0.047067	4.109728
232.840950	5770.336036	7.884659	-0.047103	4.112490
233.169574	5778.383629	7.889664	-0.047170	4.115252
233.215887	5786.355761	7.894669	-0.047183	4.117982
233.399432	5794.371176	7.899674	-0.047223	4.120727
233.579733	5802.362909	7.904678	-0.047262	4.123462
233.625818	5810.407756	7.909683	-0.047276	4.126211
233.775472	5818.420497	7.914688	-0.047309	4.128949
234.128126	5826.421423	7.919693	-0.047380	4.131684
234.450742	5834.501202	7.924698	-0.047445	4.134443
234.735908	5842.502596	7.929702	-0.047503	4.137173
235.036106	5850.445608	7.934707	-0.047564	4.139882
235.174457	5858.528901	7.939712	-0.047596	4.142634
235.161044	5866.484166	7.944717	-0.047598	4.145340
235.499301	5874.571429	7.949722	-0.047667	4.148093
235.526287	5882.541404	7.954726	-0.047677	4.150800
235.585301	5890.590050	7.959731	-0.047693	4.153533
235.952692	5898.684373	7.964736	-0.047767	4.156283
236.275738	5906.611566	7.969741	-0.047832	4.158973
236.391794	5914.672550	7.974746	-0.047859	4.161705
236.478474	5922.638375	7.979750	-0.047880	4.164403
236.624093	5930.696105	7.984755	-0.047913	4.167131
237.003815	5938.658304	7.989760	-0.047989	4.169827
237.259331	5946.725025	7.994765	-0.048042	4.172555
237.461692	5954.738720	7.999770	-0.048085	4.175263
237.598395	5962.761648	8.004774	-0.048115	4.177972
237.777337	5970.744984	8.009779	-0.048154	4.180666
238.272788	5978.831109	8.014784	-0.048252	4.183396
238.393365	5986.790693	8.019789	-0.048279	4.186078
238.474513	5994.855024	8.024794	-0.048300	4.188793
238.656215	6002.880672	8.029798	-0.048339	4.191494
239.108496	6010.987848	8.034803	-0.048428	4.194224
239.308075	6018.988248	8.039808	-0.048471	4.196913
239.491385	6026.868761	8.044813	-0.048510	4.199560
239.417634	6034.922176	8.049818	-0.048502	4.202261
239.799265	6042.892634	8.054822	-0.048578	4.204937
240.043418	6050.919950	8.059827	-0.048629	4.207629
239.928055	6058.953774	8.064832	-0.048612	4.210317
240.145875	6066.944679	8.069837	-0.048658	4.212993
240.356839	6075.030621	8.074842	-0.048703	4.215699
240.595721	6083.014507	8.079846	-0.048753	4.218369
240.845730	6091.007914	8.084851	-0.048804	4.221041
241.088807	6099.013243	8.089856	-0.048855	4.223715
241.315028	6106.991457	8.094861	-0.048902	4.226378
241.599479	6115.062179	8.099866	-0.048960	4.229071
241.765638	6123.097402	8.104870	-0.048997	4.231749
241.840843	6131.138433	8.109875	-0.049016	4.234426
241.945534	6139.220392	8.114880	-0.049041	4.237116
242.250144	6147.152725	8.119885	-0.049103	4.239756
242.406599	6155.206002	8.124890	-0.049137	4.242433
242.438414	6163.158685	8.129894	-0.049148	4.245074
242.648434	6171.147346	8.134899	-0.049193	4.247727
242.933904	6179.196541	8.139904	-0.049251	4.250398
243.150282	6187.202799	8.144909	-0.049297	4.253054
243.503225	6195.248309	8.149914	-0.049368	4.255721
243.606487	6203.289449	8.154918	-0.049392	4.258384
243.706314	6211.279112	8.159923	-0.049416	4.261028
244.055555	6219.334496	8.164928	-0.049486	4.263694
244.124506	6227.313310	8.169933	-0.049504	4.266330
244.252297	6235.367506	8.174938	-0.049534	4.268990
244.502437	6243.398180	8.179942	-0.049585	4.271642
244.712738	6251.441569	8.184947	-0.049630	4.274296
245.002596	6259.539275	8.189952	-0.049689	4.276967
245.085128	6267.432905	8.194957	-0.049710	4.279567
245.291314	6275.491594	8.199962	-0.049753	4.282221
245.585271	6283.436491	8.204966	-0.049813	4.284837
245.829390	6291.495856	8.209971	-0.049864	4.287488
246.060146	6299.480780	8.214976	-0.049912	4.290113
246.019341	6307.522695	8.219981	-0.049910	4.292753
246.488126	6315.577740	8.224986	-0.050003	4.295400
246.564304	6323.580298	8.229990	-0.050022	4.298024
246.795265	6331.589028	8.234995	-0.050070	4.300651
246.851597	6339.595252	8.240000	-0.050086	4.303273
246.981689	6347.613328	8.245005	-0.050116	4.305898
247.363352	6355.626961	8.250010	-0.050192	4.308522
247.576910	6363.637873	8.255014	-0.050237	4.311143
247.872129	6371.678740	8.260019	-0.050297	4.313772
247.860480	6379.751350	8.265024	-0.050300	4.316407
247.972693	6387.690341	8.270029	-0.050326	4.318999
248.444551	6395.728045	8.275034	-0.050420	4.321623
248.428806	6403.690994	8.280038	-0.050422	4.324218
248.499053	6411.771040	8.285043	-0.050440	4.326850
248.885957	6419.754537	8.290048	-0.050518	4.329451
248.869246	6427.783875	8.295053	-0.050520	4.332063
249.254675	6435.836830	8.300058	-0.050597	4.334684
249.356407	6443.836101	8.305062	-0.050621	4.337283
249.419926	6451.802507	8.310067	-0.050638	4.339871
249.827819	6459.874725	8.315072	-0.050719	4.342493
250.020894	6467.831950	8.320077	-0.050760	4.345075
250.032245	6475.867823	8.325082	-0.050768	4.347679
250.285681	6483.900065	8.330086	-0.050820	4.350283
250.316660	6491.956852	8.335091	-0.050831	4.352891
250.773043	6500.059794	8.340096	-0.050922	4.355516
250.896284	6507.969200	8.345101	-0.050950	4.358074
250.966557	6515.951924	8.350106	-0.050968	4.360654
251.267664	6523.971993	8.355110	-0.051029	4.363246
251.462632	6531.964988	8.360115	-0.051071	4.365827
251.789475	6540.027275	8.365120	-0.051137	4.368429
251.807638	6548.010773	8.370125	-0.051146	4.371003
252.044448	6556.047562	8.375130	-0.051195	4.373594
252.139072	6564.079036	8.380134	-0.051218	4.376180
252.174320	6572.098841	8.385139	-0.051230	4.378761
252.391561	6580.120365	8.390144	-0.051276	4.381342
252.848711	6588.064062	8.395149	-0.051366	4.383898
252.681872	6596.096629	8.400154	-0.051340	4.386477
252.941462	6604.144517	8.405158	-0.051394	4.389062
253.084440	6612.148500	8.410163	-0.051426	4.391631
253.207732	6620.208187	8.415168	-0.051454	4.394216
253.387988	6628.220147	8.420173	-0.051493	4.396784
253.578725	6636.186984	8.425178	-0.051534	4.399337
253.801356	6644.270248	8.430182	-0.051580	4.401925
253.752055	6652.239417	8.435187	-0.051576	4.404475
254.028787	6660.300214	8.440192	-0.051633	4.407053
254.341689	6668.258793	8.445197	-0.051697	4.409598
254.389838	6676.305104	8.450202	-0.051711	4.412167
254.505440	6684.361052	8.455206	-0.051738	4.414739
254.658876	6692.385978	8.460211	-0.051772	4.417299
254.846147	6700.370100	8.465216	-0.051812	4.419845
254.921976	6708.389823	8.470221	-0.051831	4.422401
255.337558	6716.383213	8.475226	-0.051914	4.424947
255.658504	6724.446414	8.480230	-0.051979	4.427515
255.554562	6732.458065	8.485235	-0.051965	4.430062
255.810353	6740.520802	8.490240	-0.052018	4.432626
255.986906	6748.505749	8.495245	-0.052056	4.435163
256.246726	6756.517927	8.500250	-0.052109	4.437708
256.497863	6764.503425	8.505254	-0.052161	4.440243
256.781086	6772.520785	8.510259	-0.052219	4.442786
256.973338	6780.526194	8.515264	-0.052261	4.445324
256.985509	6788.552146	8.520269	-0.052268	4.447866
257.143293	6796.570197	8.525274	-0.052303	4.450405
257.397026	6804.637231	8.530278	-0.052355	4.452958
257.540800	6812.623298	8.535283	-0.052387	4.455484
257.806241	6820.646250	8.540288	-0.052442	4.458020
257.918095	6828.628049	8.545293	-0.052468	4.460542
257.941846	6836.639074	8.550298	-0.052478	4.463071
258.049224	6844.641930	8.555302	-0.052503	4.465596
258.479261	6852.674866	8.560307	-0.052588	4.468130
258.600985	6860.710606	8.565312	-0.052616	4.470662
258.714631	6868.749053	8.570317	-0.052643	4.473194
258.827753	6876.795089	8.575322	-0.052669	4.475727
259.263998	6884.768309	8.580327	-0.052756	4.478237
259.420394	6892.748701	8.585331	-0.052790	4.480746
259.537475	6900.778707	8.590336	-0.052817	4.483270
259.644925	6908.768626	8.595341	-0.052842	4.485779
259.996345	6916.822705	8.600346	-0.052913	4.488308
260.091219	6924.827832	8.605351	-0.052936	4.490819
260.339818	6932.857171	8.610355	-0.052987	4.493337
260.462344	6940.896093	8.615360	-0.053016	4.495856
260.590003	6948.875719	8.620365	-0.053045	4.498355
260.838844	6956.880891	8.625370	-0.053096	4.500861
261.013063	6964.911139	8.630375	-0.053134	4.503374
261.015967	6972.890215	8.635379	-0.053140	4.505868
261.316793	6980.960636	8.640384	-0.053201	4.508390
261.484852	6988.969584	8.645389	-0.053238	4.510892
261.550063	6997.043751	8.650394	-0.053255	4.513412
261.567357	7005.080716	8.655399	-0.053264	4.515919
262.049452	7013.023182	8.660403	-0.053358	4.518396
262.303902	7021.057734	8.665408	-0.053411	4.520900
262.192837	7028.993620	8.670413	-0.053396	4.523371
262.470601	7037.013962	8.675418	-0.053453	4.525867
262.877461	7045.059253	8.680423	-0.053534	4.528371
262.870159	7053.049990	8.685427	-0.053538	4.530855
263.095590	7061.149515	8.690432	-0.053585	4.533372
263.144670	7069.131778	8.695437	-0.053599	4.535851
263.531501	7077.151130	8.700442	-0.053677	4.538340
263.561210	7085.151408	8.705447	-0.053687	4.540822
263.792018	7093.129070	8.710451	-0.053736	4.543295
264.000703	7101.162666	8.715456	-0.053780	4.545785
264.140337	7109.178825	8.720461	-0.053811	4.548268
264.529009	7117.151135	8.725466	-0.053889	4.550735
264.536406	7125.246297	8.730471	-0.053895	4.553240
264.663117	7133.249599	8.735475	-0.053924	4.555714
264.750490	7141.317051	8.740480	-0.053946	4.558207
265.161194	7149.244496	8.745485	-0.054027	4.560656
265.272775	7157.274251	8.750490	-0.054053	4.563134
265.451873	7165.288021	8.755495	-0.054092	4.565606
265.366112	7173.337161	8.760499	-0.054081	4.568088
265.850048	7181.344964	8.765504	-0.054177	4.570556
265.942784	7189.399544	8.770509	-0.054199	4.573037
266.315539	7197.398256	8.775514	-0.054274	4.575499
266.392125	7205.441415	8.780519	-0.054294	4.577974
266.500593	7213.409709	8.785523	-0.054319	4.580424
266.514077	7221.420008	8.790528	-0.054327	4.582886
266.707845	7229.426358	8.795533	-0.054368	4.585345
266.927284	7237.456405	8.800538	-0.054414	4.587810
267.181081	7245.527494	8.805543	-0.054467	4.590286
267.209731	7253.523652	8.810547	-0.054477	4.592738
267.681063	7261.577104	8.815552	-0.054570	4.595207
267.784760	7269.568726	8.820557	-0.054595	4.597654
268.046808	7277.520863	8.825562	-0.054649	4.600089
268.283255	7285.519151	8.830567	-0.054698	4.602536
268.649072	7293.516797	8.835571	-0.054772	4.604982
268.685438	7301.651328	8.840576	-0.054784	4.607468
268.750327	7309.615508	8.845581	-0.054801	4.609901
269.035887	7317.631290	8.850586	-0.054860	4.612349
269.261092	7325.638048	8.855591	-0.054907	4.614792
269.392559	7333.667405	8.860595	-0.054937	4.617241
269.760897	7341.700536	8.865600	-0.055010	4.619690
269.908307	7349.710945	8.870605	-0.055043	4.622130
269.922952	7357.658676	8.875610	-0.055051	4.624550
270.374305	7365.731767	8.880615	-0.055140	4.627007
270.606920	7373.672182	8.885619	-0.055189	4.629422
270.628623	7381.774394	8.890624	-0.055198	4.631885
270.772648	7389.778555	8.895629	-0.055230	4.634317
270.936152	7397.801447	8.900634	-0.055266	4.636754
271.076597	7405.772992	8.905639	-0.055297	4.639173
271.177234	7413.785667	8.910643	-0.055321	4.641604
271.646592	7421.796846	8.915648	-0.055414	4.644033
271.855807	7429.806173	8.920653	-0.055458	4.646460
272.066601	7437.820815	8.925658	-0.055503	4.648887
272.141368	7445.866966	8.930663	-0.055522	4.651323
272.467123	7453.858708	8.935667	-0.055588	4.653741
272.639415	7461.930393	8.940672	-0.055625	4.656181
272.632261	7469.923844	8.945677	-0.055629	4.658598
272.974081	7477.914014	8.950682	-0.055698	4.661011
273.203978	7485.964729	8.955687	-0.055746	4.663441
273.356788	7493.936516	8.960691	-0.055780	4.665847
273.714099	7502.014125	8.965696	-0.055852	4.668283
273.659464	7509.987914	8.970701	-0.055847	4.670687
273.680503	7518.099973	8.975706	-0.055856	4.673131
273.916172	7526.201107	8.980711	-0.055905	4.675570
274.028055	7534.092014	8.985715	-0.055931	4.677945
274.248251	7542.055203	8.990720	-0.055978	4.680340
274.270108	7550.083467	8.995725	-0.055987	4.682754
274.596253	7557.993423	9.000730	-0.056053	4.685130
274.858539	7566.117057	9.005735	-0.056107	4.687570
275.024795	7574.057060	9.010739	-0.056143	4.689953
275.282845	7582.125745	9.015744	-0.056197	4.692374
275.561154	7590.117651	9.020749	-0.056254	4.694770
275.610467	7598.168112	9.025754	-0.056268	4.697183
275.809051	7606.145832	9.030759	-0.056310	4.699573
276.155974	7614.174875	9.035763	-0.056380	4.701976
276.335104	7622.141984	9.040768	-0.056419	4.704360
276.302357	7630.209418	9.045773	-0.056418	4.706773
276.324518	7638.195849	9.050778	-0.056427	4.709161
276.678227	7646.239655	9.055783	-0.056499	4.711564
276.521596	7654.304730	9.060787	-0.056475	4.713973
276.838667	7662.307422	9.065792	-0.056539	4.716361
277.211892	7670.299165	9.070797	-0.056614	4.718744
277.121720	7678.298722	9.075802	-0.056602	4.721130
277.465162	7686.319407	9.080807	-0.056671	4.723520
277.786656	7694.323097	9.085811	-0.056737	4.725903
277.910208	7702.390688	9.090816	-0.056765	4.728305
278.120339	7710.355315	9.095821	-0.056809	4.730674
278.020997	7718.415029	9.100826	-0.056796	4.733072
278.396685	7726.436970	9.105831	-0.056871	4.735456
278.336813	7734.409692	9.110835	-0.056865	4.737825
278.583298	7742.452053	9.115840	-0.056917	4.740213
278.854480	7750.458894	9.120845	-0.056972	4.742588
279.030543	7758.441334	9.125850	-0.057010	4.744956
279.191868	7766.525588	9.130855	-0.057046	4.747353
279.266421	7774.498061	9.135859	-0.057065	4.749716
279.540378	7782.580401	9.140864	-0.057121	4.752109
279.649290	7790.586736	9.145869	-0.057147	4.754479
279.861982	7798.620648	9.150874	-0.057192	4.756856
280.043918	7806.549516	9.155879	-0.057231	4.759201
280.091498	7814.578774	9.160883	-0.057245	4.761574
280.333286	7822.562965	9.165888	-0.057295	4.763933
280.662995	7830.585220	9.170893	-0.057362	4.766301
280.554236	7838.610664	9.175898	-0.057347	4.768670
281.001427	7846.622668	9.180903	-0.057435	4.771032
281.263818	7854.648833	9.185907	-0.057489	4.773398
281.306734	7862.633467	9.190912	-0.057503	4.775752
281.421897	7870.702642	9.195917	-0.057529	4.778128
281.648268	7878.705464	9.200922	-0.057577	4.780484
281.995203	7886.746013	9.205927	-0.057647	4.782849
282.182226	7894.680976	9.210931	-0.057687	4.785182
282.116092	7902.789016	9.215936	-0.057680	4.787567
282.241435	7910.756438	9.220941	-0.057708	4.789907
282.545126	7918.816809	9.225946	-0.057770	4.792274
282.575976	7926.827896	9.230951	-0.057781	4.794625
282.759674	7934.799708	9.235955	-0.057821	4.796964
283.210765	7942.827881	9.240960	-0.057910	4.799316
283.457397	7950.820490	9.245965	-0.057961	4.801658
283.563282	7958.793373	9.250970	-0.057986	4.803994
283.828745	7966.892380	9.255975	-0.058041	4.806364
283.827757	7974.860667	9.260979	-0.058046	4.808697
283.895549	7982.908765	9.265984	-0.058064	4.811051
284.084719	7990.312692	9.270989	-0.058104	4.813215
284.188510	7994.871655	9.275994	-0.058126	4.814547

284.405487	7997.407260	9.280999	-0.058168	4.815287
284.467131	7998.753433	9.286003	-0.058181	4.815680
284.694586	7999.253306	9.291008	-0.058223	4.815825
284.707858	8000.138237	9.296013	-0.058226	4.816084
284.927049	8000.155046	9.301018	-0.058267	4.816087
285.197038	8000.201627	9.306023	-0.058318	4.816099
285.159991	8000.141122	9.311027	-0.058311	4.816082
285.070293	8000.175826	9.316032	-0.058294	4.816093
285.293192	8000.195908	9.321037	-0.058336	4.816097
285.435563	8000.139732	9.326042	-0.058362	4.816080
285.584415	8000.237539	9.331047	-0.058390	4.816108
285.507085	8000.181644	9.336051	-0.058376	4.816092
285.704559	8000.205539	9.341056	-0.058413	4.816098
285.661300	8000.190866	9.346061	-0.058404	4.816094
285.647261	8000.158560	9.351066	-0.058402	4.816084
285.854944	8000.222176	9.356071	-0.058441	4.816102
285.688440	8000.179619	9.361075	-0.058410	4.816090
285.779862	8000.181285	9.366080	-0.058427	4.816090
285.885168	8000.198163	9.371085	-0.058446	4.816095
285.897468	8000.155650	9.376090	-0.058449	4.816082
285.825962	8000.165040	9.381095	-0.058435	4.816085
285.787579	8000.134428	9.386099	-0.058428	4.816077
286.026252	8000.221047	9.391104	-0.058473	4.816101
286.150379	8000.152785	9.396109	-0.058496	4.816080
286.005484	8000.156566	9.401114	-0.058469	4.816082
286.133450	8000.241173	9.406119	-0.058493	4.816106
285.997934	8000.147890	9.411123	-0.058468	4.816079
286.142673	8000.170827	9.416128	-0.058495	4.816085
286.231700	8000.183135	9.421133	-0.058511	4.816089
286.131179	8000.158873	9.426138	-0.058493	4.816082
286.392826	8000.230951	9.431143	-0.058541	4.816102
286.449324	8000.173213	9.436147	-0.058552	4.816084
286.449484	8000.215962	9.441152	-0.058552	4.816097
286.368255	8000.166406	9.446157	-0.058537	4.816083
286.404084	8000.183089	9.451162	-0.058544	4.816088
286.565155	8000.225558	9.456167	-0.058574	4.816099
286.398330	8000.222529	9.461171	-0.058543	4.816099
286.375265	8000.216772	9.466176	-0.058539	4.816098
286.482812	8000.214457	9.471181	-0.058559	4.816096
286.705116	8000.209955	9.476186	-0.058600	4.816094
286.615194	8000.241449	9.481191	-0.058583	4.816104
286.532445	8000.199344	9.486195	-0.058568	4.816092
286.693782	8000.218310	9.491200	-0.058598	4.816096
286.802056	8000.300425	9.496205	-0.058618	4.816120
286.704210	8000.222783	9.501210	-0.058600	4.816098
286.829964	8000.220800	9.506215	-0.058624	4.816096
286.817617	8000.214168	9.511219	-0.058621	4.816094
286.746882	8000.212886	9.516224	-0.058608	4.816094
286.834426	8000.229442	9.521229	-0.058625	4.816099
286.861767	8000.201093	9.526234	-0.058630	4.816090
286.841782	8000.243476	9.531239	-0.058626	4.816103
286.570256	8000.221446	9.536243	-0.058575	4.816098
286.595322	8000.251826	9.541248	-0.058580	4.816107
286.600804	8000.271164	9.546253	-0.058581	4.816112
286.623141	8000.227764	9.551258	-0.058585	4.816099
286.685702	8000.241728	9.556263	-0.058597	4.816103
286.588885	8000.214327	9.561267	-0.058579	4.816096
286.698222	8000.232348	9.566272	-0.058600	4.816100
286.657010	8000.313881	9.571277	-0.058592	4.816124
286.782229	8000.225336	9.576282	-0.058615	4.816098
287.007445	8000.249738	9.581287	-0.058657	4.816104
286.789869	8000.240443	9.586291	-0.058617	4.816102
286.817274	8000.223849	9.591296	-0.058622	4.816097
286.974344	8000.264109	9.596301	-0.058651	4.816108
286.909701	8000.183865	9.601306	-0.058639	4.816085
287.019285	8000.213644	9.606311	-0.058660	4.816093
286.906889	8000.213742	9.611315	-0.058639	4.816094
286.808404	8000.244012	9.616320	-0.058621	4.816103
286.885084	8000.243274	9.621325	-0.058635	4.816103
286.917915	8000.218230	9.626330	-0.058641	4.816095
286.913427	8000.316459	9.631335	-0.058640	4.816124
287.001046	8000.184488	9.636339	-0.058657	4.816085
286.910046	8000.202071	9.641344	-0.058640	4.816090
287.054972	8000.223945	9.646349	-0.058667	4.816096
287.096025	8000.230039	9.651354	-0.058674	4.816098
287.116915	8000.271028	9.656359	-0.058678	4.816109
287.023878	8000.196679	9.661363	-0.058661	4.816088
287.067034	8000.170754	9.666368	-0.058669	4.816080
287.048782	8000.219580	9.671373	-0.058666	4.816095
287.047044	8000.190702	9.676378	-0.058665	4.816086
287.213725	8000.247165	9.681383	-0.058697	4.816102
287.253832	8000.201951	9.686387	-0.058704	4.816089
287.339479	8000.259078	9.691392	-0.058720	4.816105
287.315228	8000.307796	9.696397	-0.058716	4.816119
287.173570	8000.187682	9.701402	-0.058689	4.816085
287.364876	8000.274513	9.706407	-0.058725	4.816109
287.262072	8000.266236	9.711411	-0.058706	4.816107
287.232487	8000.266771	9.716416	-0.058700	4.816108
287.118277	8000.298892	9.721421	-0.058679	4.816118
287.279179	8000.262286	9.726426	-0.058709	4.816106
287.562578	8000.265308	9.731431	-0.058762	4.816105
287.414034	8000.256199	9.736435	-0.058734	4.816104
287.216802	8000.250480	9.741440	-0.058698	4.816103
287.296769	8000.239116	9.746445	-0.058713	4.816099
287.624828	8000.206618	9.751450	-0.058774	4.816088
287.566795	8000.281435	9.756455	-0.058763	4.816110
287.420553	8000.236037	9.761459	-0.058736	4.816098
287.536184	8000.244556	9.766464	-0.058757	4.816099
287.480245	8000.222172	9.771469	-0.058747	4.816093
287.401973	8000.181216	9.776474	-0.058732	4.816082
287.575832	8000.222850	9.781479	-0.058765	4.816093
287.471785	8000.247677	9.786483	-0.058746	4.816101
287.230797	8000.220858	9.791488	-0.058701	4.816094
287.307931	8000.240431	9.796493	-0.058715	4.816099
287.376430	8000.219241	9.801498	-0.058728	4.816093
287.354211	8000.248761	9.806503	-0.058724	4.816102
287.452373	8000.225974	9.811507	-0.058742	4.816094
287.505169	8000.245104	9.816512	-0.058752	4.816100
287.608825	8000.254474	9.821517	-0.058771	4.816102
287.362295	8000.239309	9.826522	-0.058726	4.816099
287.767335	8000.286218	9.831527	-0.058801	4.816110
287.490619	8000.272640	9.836531	-0.058750	4.816108
287.635916	8000.271013	9.841536	-0.058777	4.816107
287.493413	8000.272699	9.846541	-0.058750	4.816108
287.515612	8000.194034	9.851546	-0.058754	4.816085
287.661814	8000.255469	9.856551	-0.058782	4.816102
287.529756	8000.229562	9.861555	-0.058757	4.816095
287.784016	8000.234192	9.866560	-0.058804	4.816095
287.673002	8000.266371	9.871565	-0.058784	4.816105
287.684134	8000.228109	9.876570	-0.058786	4.816094
287.650429	8000.283066	9.881575	-0.058780	4.816110
287.461947	8000.292465	9.886579	-0.058745	4.816114
287.485033	8000.244804	9.891584	-0.058749	4.816100
287.706634	8000.261662	9.896589	-0.058790	4.816104
287.675859	8000.220501	9.901594	-0.058785	4.816092
287.748629	8000.251749	9.906599	-0.058798	4.816100
287.584539	8000.230602	9.911603	-0.058768	4.816095
287.774079	8000.260769	9.916608	-0.058803	4.816103
287.913875	8000.326363	9.921613	-0.058829	4.816121
287.694750	8000.265746	9.926618	-0.058788	4.816105
287.837790	8000.280107	9.931623	-0.058815	4.816108
287.717438	8000.337762	9.936627	-0.058793	4.816126
287.736823	8000.292170	9.941632	-0.058796	4.816112
287.754531	8000.343789	9.946637	-0.058800	4.816127
287.623139	8000.217448	9.951642	-0.058775	4.816091
287.755719	8000.271156	9.956647	-0.058800	4.816106
287.925091	8000.262487	9.961651	-0.058832	4.816103
287.765328	8000.232871	9.966656	-0.058802	4.816095
287.800109	8000.309376	9.971661	-0.058808	4.816117
287.818180	8000.257349	9.976666	-0.058812	4.816102
287.897637	8000.286582	9.981671	-0.058827	4.816110
287.729450	8000.268567	9.986675	-0.058795	4.816105
287.804678	8000.293448	9.991680	-0.058809	4.816112
287.841989	8000.290926	9.996685	-0.058816	4.816111
288.083443	8000.249374	10.001690	-0.058861	4.816098
288.150546	8000.305097	10.006695	-0.058874	4.816114
288.089081	8000.267651	10.011699	-0.058863	4.816103
288.069664	8000.259822	10.016704	-0.058859	4.816101
288.017570	8000.314445	10.021709	-0.058849	4.816117
287.989897	8000.255174	10.026714	-0.058844	4.816100
288.193179	8000.258877	10.031719	-0.058882	4.816100
287.977725	8000.264579	10.036723	-0.058842	4.816103
287.886272	8000.269331	10.041728	-0.058825	4.816105
287.923968	8000.268952	10.046733	-0.058832	4.816104
288.030632	8000.249525	10.051738	-0.058852	4.816098
287.952397	8000.340005	10.056743	-0.058838	4.816125
287.807136	8000.268977	10.061747	-0.058810	4.816105
287.994273	8000.274523	10.066752	-0.058845	4.816106
288.170119	8000.272384	10.071757	-0.058878	4.816104
287.937525	8000.264951	10.076762	-0.058835	4.816103
288.147685	8000.286945	10.081767	-0.058874	4.816109
288.081755	8000.297504	10.086771	-0.058862	4.816112
288.010690	8000.278049	10.091776	-0.058849	4.816107
288.151503	8000.307330	10.096781	-0.058875	4.816114
288.180487	8000.266187	10.101786	-0.058880	4.816102
288.335930	8000.314969	10.106791	-0.058909	4.816116
288.272496	8000.383278	10.111795	-0.058898	4.816136
288.390058	8000.334129	10.116800	-0.058920	4.816121
288.196385	8000.307100	10.121805	-0.058884	4.816114
288.071048	8000.321922	10.126810	-0.058860	4.816119
288.103400	8000.328926	10.131815	-0.058866	4.816121
288.044382	8000.318239	10.136819	-0.058855	4.816118
288.071083	8000.285603	10.141824	-0.058860	4.816109
288.146330	8000.364984	10.146829	-0.058874	4.816131
288.232756	8000.289622	10.151834	-0.058891	4.816109
288.331737	8000.279673	10.156839	-0.058909	4.816105
288.266009	8000.307333	10.161843	-0.058897	4.816114
288.352146	8000.254407	10.166848	-0.058913	4.816098
288.206772	8000.267795	10.171853	-0.058886	4.816103
288.111064	8000.275676	10.176858	-0.058868	4.816105
288.145804	8000.334016	10.181863	-0.058875	4.816122
288.277276	8000.247719	10.186867	-0.058899	4.816096
288.177604	8000.242705	10.191872	-0.058881	4.816095
288.208669	8000.318075	10.196877	-0.058886	4.816117
288.278463	8000.218902	10.201882	-0.058899	4.816088
288.544104	8000.317776	10.206887	-0.058949	4.816115
288.163844	8000.321547	10.211891	-0.058878	4.816118
288.177518	8000.268371	10.216896	-0.058881	4.816103
288.405357	8000.336636	10.221901	-0.058923	4.816122
288.278586	8000.281973	10.226906	-0.058900	4.816106
288.293529	8000.307895	10.231911	-0.058903	4.816114
288.276369	8000.299039	10.236915	-0.058899	4.816111
288.304889	8000.270710	10.241920	-0.058905	4.816103
288.474122	8000.256696	10.246925	-0.058936	4.816098
288.221361	8000.240347	10.251930	-0.058889	4.816094
288.429350	8000.321075	10.256935	-0.058928	4.816117
288.212157	8000.277589	10.261939	-0.058888	4.816105
288.348416	8000.298239	10.266944	-0.058913	4.816111
288.529509	8000.316499	10.271949	-0.058947	4.816115
288.318404	8000.254958	10.276954	-0.058908	4.816098
288.531584	8000.349672	10.281959	-0.058947	4.816125
288.544191	8000.316779	10.286963	-0.058950	4.816115
288.343827	8000.240473	10.291968	-0.058912	4.816094
288.365420	8000.297506	10.296973	-0.058917	4.816110
288.353847	8000.294094	10.301978	-0.058914	4.816109
288.327122	8000.278652	10.306983	-0.058910	4.816105
288.212129	8000.257329	10.311987	-0.058888	4.816099
288.262197	8000.232599	10.316992	-0.058897	4.816092
288.367425	8000.294359	10.321997	-0.058917	4.816109
288.224682	8000.244748	10.327002	-0.058891	4.816096
288.421175	8000.271836	10.332007	-0.058927	4.816103
288.495209	8000.271051	10.337011	-0.058941	4.816102
288.522865	8000.235226	10.342016	-0.058946	4.816091
288.367274	8000.278349	10.347021	-0.058917	4.816105
288.446777	8000.279800	10.352026	-0.058932	4.816105
288.763729	8000.299464	10.357031	-0.058991	4.816109
288.563683	8000.274456	10.362035	-0.058954	4.816103
288.525525	8000.262011	10.367040	-0.058947	4.816099
288.493519	8000.347989	10.372045	-0.058941	4.816124
288.418020	8000.293190	10.377050	-0.058927	4.816109
288.540844	8000.267646	10.382055	-0.058950	4.816101
288.506997	8000.333287	10.387059	-0.058944	4.816120
288.540621	8000.306120	10.392064	-0.058950	4.816112
288.383852	8000.311821	10.397069	-0.058921	4.816114
288.288738	8000.291928	10.402074	-0.058903	4.816109
288.507046	8000.329031	10.407079	-0.058944	4.816119
288.372222	8000.314828	10.412083	-0.058919	4.816115
288.507553	8000.278825	10.417088	-0.058944	4.816104
288.723656	8000.331918	10.422093	-0.058984	4.816118
288.652347	8000.292155	10.427098	-0.058971	4.816107
288.671754	8000.285032	10.432103	-0.058975	4.816105
288.655961	8000.312533	10.437107	-0.058972	4.816113
288.641679	8000.274876	10.442112	-0.058969	4.816102
288.676871	8000.293687	10.447117	-0.058976	4.816108
288.547399	8000.225083	10.452122	-0.058952	4.816088
288.690802	8000.300361	10.457127	-0.058979	4.816109
288.702163	8000.316601	10.462131	-0.058981	4.816114
288.618943	8000.296925	10.467136	-0.058965	4.816109
288.808572	8000.323890	10.472141	-0.059001	4.816116
288.805028	8000.309938	10.477146	-0.059000	4.816112
288.679507	8000.317275	10.482151	-0.058977	4.816114
288.654163	8000.289035	10.487155	-0.058972	4.816106
288.580478	8000.277012	10.492160	-0.058958	4.816103
288.743510	8000.260749	10.497165	-0.058989	4.816098
288.618312	8000.206114	10.502170	-0.058965	4.816082
288.822057	8000.234403	10.507175	-0.059003	4.816089
288.637658	8000.237464	10.512179	-0.058969	4.816091
288.792786	8000.241359	10.517184	-0.058998	4.816092
288.915098	8000.302363	10.522189	-0.059021	4.816109
288.976468	8000.237231	10.527194	-0.059032	4.816089
288.775812	8000.244269	10.532199	-0.058995	4.816093
288.712674	8000.295486	10.537203	-0.058983	4.816108
288.696165	8000.295190	10.542208	-0.058980	4.816108
288.693578	8000.299422	10.547213	-0.058980	4.816109
288.675389	8000.270243	10.552218	-0.058977	4.816101
288.720185	8000.292435	10.557223	-0.058985	4.816107
288.904979	8000.278704	10.562227	-0.059019	4.816102
288.766581	8000.252681	10.567232	-0.058994	4.816095
288.856712	8000.323785	10.572237	-0.059011	4.816115
288.781047	8000.323481	10.577242	-0.058996	4.816116
288.969966	8000.344021	10.582247	-0.059032	4.816121
288.893601	8000.364008	10.587251	-0.059018	4.816127
288.820968	8000.291094	10.592256	-0.059004	4.816106
288.843556	8000.303264	10.597261	-0.059008	4.816109
288.874991	8000.257890	10.602266	-0.059014	4.816096
288.977977	8000.331366	10.607271	-0.059033	4.816117
288.932750	8000.355125	10.612275	-0.059025	4.816124
288.620241	8000.275708	10.617280	-0.058967	4.816103
288.782503	8000.337438	10.622285	-0.058997	4.816120
288.947881	8000.287022	10.627290	-0.059028	4.816104
288.798050	8000.308878	10.632295	-0.059000	4.816111
288.729642	8000.278785	10.637299	-0.058987	4.816103
288.803033	8000.252341	10.642304	-0.059001	4.816095
288.812718	8000.290992	10.647309	-0.059003	4.816106
288.647371	8000.269821	10.652314	-0.058972	4.816101
288.791665	8000.300235	10.657319	-0.058999	4.816109
288.930593	8000.359404	10.662323	-0.059025	4.816125
288.621452	8000.283254	10.667328	-0.058968	4.816105
288.610415	8000.321527	10.672333	-0.058966	4.816116
288.764574	8000.235643	10.677338	-0.058994	4.816090
288.849682	8000.267117	10.682343	-0.059010	4.816099
288.969692	8000.274649	10.687347	-0.059033	4.816100
288.979380	8000.282310	10.692352	-0.059034	4.816103
288.934295	8000.340267	10.697357	-0.059026	4.816120
288.911874	8000.300325	10.702362	-0.059022	4.816108
288.980104	8000.356070	10.707367	-0.059035	4.816124
289.046107	8000.314531	10.712371	-0.059047	4.816112
288.816923	8000.216327	10.717376	-0.059004	4.816084
288.985943	8000.308102	10.722381	-0.059036	4.816110
288.893501	8000.280777	10.727386	-0.059019	4.816103
289.127227	8000.336329	10.732391	-0.059062	4.816118
288.945175	8000.320196	10.737395	-0.059028	4.816114
289.086370	8000.277889	10.742400	-0.059055	4.816101
289.191747	8000.326830	10.747405	-0.059074	4.816114
288.942492	8000.274210	10.752410	-0.059028	4.816100
289.037219	8000.304791	10.757415	-0.059046	4.816109
289.084117	8000.324884	10.762419	-0.059055	4.816114
289.242568	8000.240147	10.767424	-0.059084	4.816089
289.110039	8000.281552	10.772429	-0.059059	4.816102
289.075866	8000.290552	10.777434	-0.059053	4.816104
289.220871	8000.282509	10.782439	-0.059080	4.816101
288.826626	8000.247555	10.787443	-0.059007	4.816093
288.806685	8000.224755	10.792448	-0.059003	4.816087
289.072248	8000.308670	10.797453	-0.059053	4.816110
288.822858	8000.272077	10.802458	-0.059006	4.816100
288.828572	8000.255088	10.807463	-0.059007	4.816095
288.924316	8000.256834	10.812467	-0.059025	4.816095
288.887277	8000.254028	10.817472	-0.059018	4.816095
288.905303	8000.267183	10.822477	-0.059022	4.816099
288.945933	8000.192056	10.827482	-0.059029	4.816076
289.328624	8000.232152	10.832487	-0.059101	4.816086
289.057750	8000.271039	10.837491	-0.059050	4.816099
289.118690	8000.239026	10.842496	-0.059062	4.816089
289.229336	8000.316916	10.847501	-0.059082	4.816111
288.997585	8000.248585	10.852506	-0.059039	4.816093
289.083677	8000.245882	10.857511	-0.059055	4.816091
289.119517	8000.251882	10.862515	-0.059062	4.816093
288.969200	8000.233122	10.867520	-0.059034	4.816088
288.901353	8000.289596	10.872525	-0.059022	4.816105
288.834607	8000.248847	10.877530	-0.059009	4.816094
288.945265	8000.293610	10.882535	-0.059030	4.816106
288.885666	8000.224139	10.887539	-0.059019	4.816086
288.975041	8000.181957	10.892544	-0.059035	4.816073
289.195848	8000.238341	10.897549	-0.059077	4.816089
289.002830	8000.233764	10.902554	-0.059041	4.816088
289.100419	8000.239819	10.907559	-0.059059	4.816089
289.088607	8000.252432	10.912563	-0.059057	4.816093
289.021187	8000.239454	10.917568	-0.059044	4.816090
289.061709	8000.307519	10.922573	-0.059052	4.816109
288.997687	8000.281780	10.927578	-0.059040	4.816102
289.302290	8000.289466	10.932583	-0.059097	4.816103
289.168260	8000.295579	10.937587	-0.059072	4.816105
288.987019	8000.242060	10.942592	-0.059038	4.816091
289.240284	8000.299036	10.947597	-0.059085	4.816106
289.096201	8000.295349	10.952602	-0.059059	4.816106
289.052040	8000.291344	10.957607	-0.059050	4.816105
289.019645	8000.286484	10.962611	-0.059044	4.816104
289.262936	8000.273819	10.967616	-0.059090	4.816099
289.054025	8000.341618	10.972621	-0.059051	4.816119
288.937759	8000.264704	10.977626	-0.059029	4.816098
289.159337	8000.250575	10.982631	-0.059070	4.816092
289.137810	8000.239501	10.987635	-0.059067	4.816089
289.012574	8000.188070	10.992640	-0.059043	4.816075
289.149503	8000.301702	10.997645	-0.059069	4.816107
289.306248	8000.232962	11.002650	-0.059098	4.816086
289.269535	8000.301758	11.007655	-0.059091	4.816107
289.311044	8000.312136	11.012659	-0.059099	4.816109
289.267471	8000.237613	11.017664	-0.059091	4.816088
289.240607	8000.336509	11.022669	-0.059086	4.816117
289.221576	8000.300903	11.027674	-0.059083	4.816107
289.212777	8000.268689	11.032679	-0.059081	4.816097
289.105766	8000.309490	11.037683	-0.059061	4.816110
289.205732	8000.295285	11.042688	-0.059080	4.816105
289.321285	8000.378607	11.047693	-0.059101	4.816129
289.409637	8000.254123	11.052698	-0.059118	4.816092
289.333228	8000.257011	11.057703	-0.059104	4.816093
289.272579	8000.293313	11.062707	-0.059092	4.816104
289.368147	8000.277959	11.067712	-0.059110	4.816099
289.444883	8000.291115	11.072717	-0.059124	4.816103
289.272658	8000.281573	11.077722	-0.059092	4.816101
289.328093	8000.272969	11.082727	-0.059103	4.816098
289.336984	8000.328703	11.087731	-0.059105	4.816114
289.219368	8000.270998	11.092736	-0.059083	4.816098
289.422170	8000.314233	11.097741	-0.059121	4.816109
289.294311	8000.286263	11.102746	-0.059097	4.816102
289.668151	8000.310171	11.107751	-0.059166	4.816107
289.362896	8000.351638	11.112755	-0.059110	4.816121
289.318795	8000.278173	11.117760	-0.059101	4.816099
289.366427	8000.290799	11.122765	-0.059110	4.816103
289.237415	8000.292730	11.127770	-0.059086	4.816104
289.638369	8000.354533	11.132775	-0.059161	4.816120
289.710821	8000.341964	11.137779	-0.059175	4.816116
289.419471	8000.280028	11.142784	-0.059120	4.816099
289.411784	8000.311951	11.147789	-0.059119	4.816109
289.646236	8000.317292	11.152794	-0.059163	4.816109
289.685155	8000.334034	11.157799	-0.059170	4.816114
289.524427	8000.340730	11.162803	-0.059140	4.816117
289.525507	8000.307627	11.167808	-0.059140	4.816107
289.572563	8000.357645	11.172813	-0.059149	4.816121
289.407104	8000.346088	11.177818	-0.059118	4.816119
289.500629	8000.278334	11.182823	-0.059136	4.816099
289.542794	8000.318645	11.187827	-0.059144	4.816110
289.433534	8000.261092	11.192832	-0.059123	4.816094
289.492412	8000.324148	11.197837	-0.059134	4.816112
289.453303	8000.321304	11.202842	-0.059127	4.816111
289.553059	8000.307095	11.207847	-0.059146	4.816107
289.600055	8000.321847	11.212851	-0.059155	4.816111
289.556231	8000.259073	11.217856	-0.059147	4.816093
289.728099	8000.308157	11.222861	-0.059179	4.816106
289.386471	8000.352168	11.227866	-0.059115	4.816121
289.561037	8000.356419	11.232871	-0.059148	4.816121
289.594284	8000.302528	11.237875	-0.059154	4.816105
289.572450	8000.251910	11.242880	-0.059150	4.816090
289.688556	8000.334175	11.247885	-0.059171	4.816114
289.745443	8000.314911	11.252890	-0.059182	4.816108
289.568959	8000.257203	11.257895	-0.059149	4.816092
289.541620	8000.334719	11.262899	-0.059144	4.816115
289.622432	8000.291312	11.267904	-0.059159	4.816102
289.752853	8000.318269	11.272909	-0.059184	4.816109
289.409384	8000.267139	11.277914	-0.059120	4.816096
289.437575	8000.280480	11.282919	-0.059125	4.816099
289.479773	8000.288733	11.287923	-0.059133	4.816102
289.574776	8000.247722	11.292928	-0.059151	4.816089
289.585714	8000.309905	11.297933	-0.059153	4.816107
289.493329	8000.266551	11.302938	-0.059136	4.816095
289.616523	8000.299789	11.307943	-0.059159	4.816104
289.528954	8000.317434	11.312947	-0.059142	4.816110
289.626222	8000.235857	11.317952	-0.059160	4.816085
289.620697	8000.345829	11.322957	-0.059160	4.816118
289.624689	8000.296749	11.327962	-0.059160	4.816103
289.642214	8000.333406	11.332967	-0.059164	4.816114
289.874858	8000.331234	11.337971	-0.059207	4.816112
289.701600	8000.324878	11.342976	-0.059175	4.816111
289.760617	8000.363359	11.347981	-0.059186	4.816122
289.790263	8000.342530	11.352986	-0.059191	4.816116
289.744403	8000.307504	11.357991	-0.059183	4.816106
289.588446	8000.335659	11.362995	-0.059154	4.816115
289.600574	8000.312374	11.368000	-0.059156	4.816108
289.598189	8000.348669	11.373005	-0.059156	4.816118
289.568904	8000.323561	11.378010	-0.059150	4.816111
289.481885	8000.341217	11.383015	-0.059134	4.816117
289.742276	8000.368403	11.388019	-0.059183	4.816123
289.680312	8000.263622	11.393024	-0.059171	4.816093
289.628240	8000.304355	11.398029	-0.059162	4.816105
289.656666	8000.265338	11.403034	-0.059167	4.816094
289.819522	8000.261895	11.408039	-0.059197	4.816092
289.963109	8000.329701	11.413043	-0.059224	4.816111
289.803121	8000.281909	11.418048	-0.059194	4.816098
289.832614	8000.334814	11.423053	-0.059200	4.816113
289.812468	8000.325902	11.428058	-0.059196	4.816111
289.678946	8000.291417	11.433063	-0.059171	4.816101
289.771846	8000.312348	11.438067	-0.059189	4.816107
289.585284	8000.229878	11.443072	-0.059154	4.816084
289.872021	8000.319524	11.448077	-0.059207	4.816109
289.872630	8000.271451	11.453082	-0.059208	4.816094
289.701943	8000.264073	11.458087	-0.059176	4.816093
289.546431	8000.374521	11.463091	-0.059147	4.816126
289.545434	8000.306115	11.468096	-0.059147	4.816106
289.995448	8000.378431	11.473101	-0.059231	4.816125
289.790622	8000.371499	11.478106	-0.059193	4.816124
289.638153	8000.338806	11.483111	-0.059164	4.816115
289.661639	8000.318934	11.488115	-0.059169	4.816109
289.767712	8000.236448	11.493120	-0.059188	4.816085
289.717399	8000.321027	11.498125	-0.059179	4.816110
289.751476	8000.284250	11.503130	-0.059185	4.816099
289.801762	8000.309748	11.508135	-0.059195	4.816106
289.856415	8000.359904	11.513139	-0.059205	4.816120
289.757465	8000.283303	11.518144	-0.059187	4.816099
289.889720	8000.377618	11.523149	-0.059211	4.816125
289.883653	8000.313394	11.528154	-0.059210	4.816107
289.741280	8000.337522	11.533159	-0.059184	4.816114
289.811487	8000.345216	11.538163	-0.059197	4.816116
289.883467	8000.280276	11.543168	-0.059210	4.816097
289.871150	8000.324938	11.548173	-0.059208	4.816110
289.859719	8000.340764	11.553178	-0.059206	4.816115
289.994362	8000.321848	11.558183	-0.059231	4.816109
289.884114	8000.344423	11.563187	-0.059211	4.816116
289.541626	8000.290104	11.568192	-0.059147	4.816102
289.956572	8000.313692	11.573197	-0.059224	4.816106
289.709077	8000.312396	11.578202	-0.059178	4.816107
289.653891	8000.292161	11.583207	-0.059168	4.816102
289.711799	8000.340239	11.588211	-0.059179	4.816115
289.861366	8000.316251	11.593216	-0.059207	4.816108
289.961845	8000.380066	11.598221	-0.059226	4.816126
289.685825	8000.347260	11.603226	-0.059174	4.816118
289.756094	8000.284426	11.608231	-0.059187	4.816099
289.917764	8000.327981	11.613235	-0.059217	4.816111
289.870175	8000.263001	11.618240	-0.059209	4.816092
289.969033	8000.310757	11.623245	-0.059227	4.816105
289.759103	8000.295184	11.628250	-0.059188	4.816102
289.755117	8000.265194	11.633255	-0.059187	4.816093
289.991545	8000.282327	11.638259	-0.059231	4.816097
289.891147	8000.245238	11.643264	-0.059213	4.816087
289.873785	8000.346447	11.648269	-0.059210	4.816116
289.938677	8000.345495	11.653274	-0.059222	4.816116
290.041098	8000.303551	11.658279	-0.059241	4.816103
289.921438	8000.305651	11.663283	-0.059219	4.816104
289.920711	8000.265034	11.668288	-0.059218	4.816092
289.964283	8000.307508	11.673293	-0.059227	4.816104
289.958021	8000.298850	11.678298	-0.059225	4.816102
289.868300	8000.295083	11.683303	-0.059209	4.816101
289.880705	8000.334853	11.688307	-0.059211	4.816113
290.002635	8000.325322	11.693312	-0.059234	4.816109
290.183114	8000.361741	11.698317	-0.059268	4.816119
289.869026	8000.299388	11.703322	-0.059209	4.816103
289.980908	8000.316391	11.708327	-0.059230	4.816107
289.809072	8000.375247	11.713331	-0.059198	4.816125
289.862317	8000.311034	11.718336	-0.059208	4.816106
289.884834	8000.298625	11.723341	-0.059212	4.816102
289.926737	8000.309010	11.728346	-0.059220	4.816105
289.835687	8000.295602	11.733351	-0.059203	4.816102
289.963833	8000.343891	11.738355	-0.059227	4.816115
290.151741	8000.286404	11.743360	-0.059262	4.816097
290.065051	8000.284830	11.748365	-0.059246	4.816097
289.980226	8000.274741	11.753370	-0.059230	4.816095
290.066199	8000.253869	11.758375	-0.059246	4.816088
290.101223	8000.268404	11.763379	-0.059253	4.816092
289.920787	8000.246956	11.768384	-0.059219	4.816087
289.994290	8000.285701	11.773389	-0.059233	4.816098
290.050832	8000.237578	11.778394	-0.059244	4.816084
290.097439	8000.266215	11.783399	-0.059252	4.816092
290.062541	8000.362830	11.788403	-0.059246	4.816120
289.904166	8000.258430	11.793408	-0.059216	4.816090
289.864870	8000.309014	11.798413	-0.059209	4.816105
289.857972	8000.295000	11.803418	-0.059208	4.816101
289.900597	8000.248761	11.808423	-0.059216	4.816088
289.846620	8000.264881	11.813427	-0.059206	4.816093
289.934512	8000.271828	11.818432	-0.059222	4.816094
289.974667	8000.324927	11.823437	-0.059230	4.816109
289.926281	8000.337942	11.828442	-0.059221	4.816114
289.863584	8000.307952	11.833447	-0.059209	4.816105
289.852794	8000.320584	11.838451	-0.059207	4.816109
289.991085	8000.224792	11.843456	-0.059233	4.816080
290.028422	8000.312035	11.848461	-0.059240	4.816105
290.013414	8000.317110	11.853466	-0.059237	4.816107
289.893870	8000.293565	11.858471	-0.059215	4.816101
289.971535	8000.311013	11.863475	-0.059230	4.816105
289.908176	8000.283147	11.868480	-0.059218	4.816098
289.922538	8000.369973	11.873485	-0.059221	4.816123
289.882932	8000.352158	11.878490	-0.059213	4.816118
289.876831	8000.267629	11.883495	-0.059212	4.816093
290.065704	8000.368318	11.888499	-0.059247	4.816122
289.979587	8000.293019	11.893504	-0.059231	4.816100
290.196090	8000.261700	11.898509	-0.059272	4.816090
290.077374	8000.301220	11.903514	-0.059250	4.816102
290.019617	8000.304447	11.908519	-0.059239	4.816103
290.159708	8000.382876	11.913523	-0.059265	4.816125
290.178685	8000.334068	11.918528	-0.059269	4.816111
290.131028	8000.318244	11.923533	-0.059260	4.816107
290.058796	8000.288080	11.928538	-0.059246	4.816098
290.039641	8000.250333	11.933543	-0.059243	4.816087
289.946650	8000.327723	11.938547	-0.059226	4.816110
290.091112	8000.257691	11.943552	-0.059253	4.816089
290.226889	8000.266579	11.948557	-0.059278	4.816091
289.843069	8000.299135	11.953562	-0.059207	4.816103
289.887640	8000.265754	11.958567	-0.059215	4.816093
290.017298	8000.301247	11.963571	-0.059239	4.816102
289.934268	8000.234553	11.968576	-0.059224	4.816083
290.013067	8000.249884	11.973581	-0.059238	4.816087
289.995166	8000.288034	11.978586	-0.059235	4.816099
289.941264	8000.267821	11.983591	-0.059225	4.816093
289.968807	8000.279013	11.988595	-0.059230	4.816096
289.971347	8000.255554	11.993600	-0.059231	4.816089
290.256164	8000.317382	11.998605	-0.059284	4.816106
290.056313	8000.311610	12.003610	-0.059247	4.816105
289.990771	8000.293323	12.008615	-0.059235	4.816100
290.094172	8000.285592	12.013619	-0.059254	4.816097
290.056669	8000.213315	12.018624	-0.059247	4.816076
290.085851	8000.310028	12.023629	-0.059252	4.816104
290.056675	8000.336217	12.028634	-0.059247	4.816112
289.948744	8000.295786	12.033639	-0.059227	4.816101
290.052833	8000.300891	12.038643	-0.059246	4.816102
290.007340	8000.265871	12.043648	-0.059238	4.816092
290.159575	8000.295363	12.048653	-0.059266	4.816100
290.095262	8000.315569	12.053658	-0.059254	4.816106
290.139036	8000.337743	12.058663	-0.059263	4.816112
290.161433	8000.374489	12.063667	-0.059267	4.816123
289.999978	8000.304229	12.068672	-0.059237	4.816103
290.059084	8000.302104	12.073677	-0.059248	4.816102
290.236484	8000.350222	12.078682	-0.059281	4.816115
290.089942	8000.278096	12.083687	-0.059254	4.816095
289.995738	8000.312719	12.088691	-0.059236	4.816106
289.951311	8000.249934	12.093696	-0.059228	4.816088
290.133400	8000.320577	12.098701	-0.059262	4.816107
289.937773	8000.267863	12.103706	-0.059225	4.816093
289.949797	8000.222135	12.108711	-0.059228	4.816079
290.173976	8000.318124	12.113715	-0.059270	4.816106
290.138763	8000.302526	12.118720	-0.059263	4.816102
290.095650	8000.365864	12.123725	-0.059255	4.816121
290.309376	8000.371897	12.128730	-0.059295	4.816121
290.304390	8000.260672	12.133735	-0.059294	4.816089
290.244268	8000.348279	12.138739	-0.059283	4.816115
290.211686	8000.269679	12.143744	-0.059277	4.816092
290.309387	8000.251158	12.148749	-0.059295	4.816086
290.207927	8000.255727	12.153754	-0.059276	4.816088
290.069757	8000.239323	12.158759	-0.059251	4.816084
290.183308	8000.303376	12.163763	-0.059272	4.816102
290.274374	8000.294353	12.168768	-0.059289	4.816099
290.217309	8000.346750	12.173773	-0.059278	4.816114
290.102814	8000.310473	12.178778	-0.059257	4.816104
290.166916	8000.265693	12.183783	-0.059269	4.816091
290.130577	8000.309918	12.188787	-0.059262	4.816104
289.914528	8000.253626	12.193792	-0.059222	4.816089
290.035077	8000.301776	12.198797	-0.059244	4.816102
290.137969	8000.304723	12.203802	-0.059264	4.816103
290.023070	8000.279125	12.208807	-0.059242	4.816096
289.995488	8000.373736	12.213811	-0.059237	4.816123
290.076187	8000.317503	12.218816	-0.059252	4.816107
290.076639	8000.284388	12.223821	-0.059252	4.816097
289.982716	8000.291232	12.228826	-0.059235	4.816099
290.052428	8000.275407	12.233831	-0.059248	4.816094
290.289241	8000.264763	12.238835	-0.059292	4.816090
290.159997	8000.243178	12.243840	-0.059268	4.816084
290.173360	8000.271210	12.248845	-0.059271	4.816093
290.021340	8000.327222	12.253850	-0.059242	4.816110
289.904431	8000.277009	12.258855	-0.059221	4.816096
290.167920	8000.436764	12.263859	-0.059270	4.816141
290.131914	8000.453211	12.268864	-0.059263	4.816146
289.995807	8000.431501	12.273869	-0.059238	4.816140
289.966982	8000.372205	12.278874	-0.059233	4.816123
290.109610	8000.317100	12.283879	-0.059259	4.816106
290.155802	8000.322220	12.288883	-0.059268	4.816108
290.019597	8000.253489	12.293888	-0.059242	4.816088
289.931519	8000.311733	12.298893	-0.059226	4.816106
290.168448	8000.335288	12.303898	-0.059270	4.816111
290.024766	8000.277106	12.308903	-0.059244	4.816095
290.022853	8000.231125	12.313907	-0.059243	4.816082
290.000992	8000.225388	12.318912	-0.059239	4.816080
290.197384	8000.296292	12.323917	-0.059276	4.816100
290.066958	8000.320638	12.328922	-0.059252	4.816108
290.200575	8000.287810	12.333927	-0.059276	4.816097
290.276638	8000.306298	12.338931	-0.059291	4.816102
290.298373	8000.285325	12.343936	-0.059295	4.816096
290.224924	8000.318188	12.348941	-0.059281	4.816106
290.410777	8000.383559	12.353946	-0.059316	4.816124
290.252466	8000.290914	12.358951	-0.059286	4.816098
290.170017	8000.350330	12.363955	-0.059271	4.816116
290.105946	8000.308559	12.368960	-0.059259	4.816104
290.154121	8000.330813	12.373965	-0.059268	4.816110
290.159936	8000.367257	12.378970	-0.059269	4.816121
290.330022	8000.319064	12.383975	-0.059301	4.816106
290.442304	8000.348898	12.388979	-0.059322	4.816114
290.413655	8000.351587	12.393984	-0.059317	4.816115
290.403374	8000.301178	12.398989	-0.059315	4.816100
290.378183	8000.311410	12.403994	-0.059310	4.816103
290.313768	8000.278182	12.408999	-0.059298	4.816094
290.412174	8000.343028	12.414003	-0.059317	4.816112
290.313284	8000.301692	12.419008	-0.059298	4.816101
290.459266	8000.373817	12.424013	-0.059326	4.816121
290.324895	8000.320079	12.429018	-0.059301	4.816106
290.257123	8000.295339	12.434023	-0.059288	4.816099
290.360075	8000.363474	12.439027	-0.059307	4.816118
290.402805	8000.309756	12.444032	-0.059315	4.816103
290.450108	8000.311690	12.449037	-0.059324	4.816103
290.294289	8000.367633	12.454042	-0.059295	4.816120
290.352216	8000.283200	12.459047	-0.059306	4.816095
290.320884	8000.348890	12.464051	-0.059300	4.816114
290.332006	8000.291390	12.469056	-0.059302	4.816098
290.534142	8000.337822	12.474061	-0.059340	4.816110
290.434557	8000.383033	12.479066	-0.059321	4.816124
290.433597	8000.311420	12.484071	-0.059321	4.816103
290.512550	8000.387668	12.489075	-0.059336	4.816125
290.549924	8000.352019	12.494080	-0.059343	4.816114
290.528460	8000.345221	12.499085	-0.059339	4.816112
290.394187	8000.308583	12.504090	-0.059314	4.816102
290.492161	8000.264420	12.509095	-0.059332	4.816089
290.492673	8000.348857	12.514099	-0.059333	4.816114
290.415051	8000.279054	12.519104	-0.059318	4.816094
290.432052	8000.338143	12.524109	-0.059321	4.816111
290.272506	8000.298908	12.529114	-0.059292	4.816100
290.285053	8000.253190	12.534119	-0.059294	4.816087
290.441708	8000.269939	12.539123	-0.059323	4.816091
290.490190	8000.294336	12.544128	-0.059332	4.816098
290.525682	8000.317429	12.549133	-0.059339	4.816104
290.519121	8000.364334	12.554138	-0.059338	4.816118
290.434310	8000.312568	12.559143	-0.059322	4.816103
290.594356	8000.363576	12.564147	-0.059352	4.816117
290.376653	8000.330762	12.569152	-0.059311	4.816109
290.507516	8000.321395	12.574157	-0.059336	4.816105
290.376113	8000.332898	12.579162	-0.059311	4.816109
290.483076	8000.280350	12.584167	-0.059331	4.816094
290.423938	8000.311336	12.589171	-0.059320	4.816103
290.408990	8000.276872	12.594176	-0.059318	4.816093
290.335478	8000.312940	12.599181	-0.059304	4.816104
290.345095	8000.348385	12.604186	-0.059306	4.816114
290.171971	8000.273638	12.609191	-0.059274	4.816093
290.184380	8000.304858	12.614195	-0.059276	4.816102
290.369186	8000.272963	12.619200	-0.059310	4.816092
290.522813	8000.308893	12.624205	-0.059339	4.816102
290.573907	8000.305553	12.629210	-0.059349	4.816100
290.464161	8000.304628	12.634215	-0.059328	4.816101
290.587090	8000.376333	12.639219	-0.059351	4.816121
290.381684	8000.288173	12.644224	-0.059313	4.816096
290.302854	8000.301703	12.649229	-0.059298	4.816101
290.422187	8000.330597	12.654234	-0.059321	4.816109
290.453783	8000.321559	12.659239	-0.059327	4.816106
290.621481	8000.319274	12.664243	-0.059358	4.816104
290.338388	8000.286338	12.669248	-0.059305	4.816096
290.491335	8000.382101	12.674253	-0.059334	4.816123
290.370500	8000.375630	12.679258	-0.059311	4.816122
290.385708	8000.318204	12.684263	-0.059314	4.816105
290.646776	8000.338993	12.689267	-0.059363	4.816110
290.361598	8000.325254	12.694272	-0.059310	4.816107
290.422635	8000.325301	12.699277	-0.059321	4.816107
290.639988	8000.403002	12.704282	-0.059362	4.816128
290.674177	8000.251880	12.709287	-0.059368	4.816084
290.592507	8000.305967	12.714291	-0.059353	4.816100
290.426052	8000.286910	12.719296	-0.059322	4.816096
290.527923	8000.327241	12.724301	-0.059341	4.816107
290.475222	8000.382924	12.729306	-0.059331	4.816123
290.473129	8000.305947	12.734311	-0.059331	4.816101
290.643002	8000.341105	12.739315	-0.059363	4.816110
290.596124	8000.342393	12.744320	-0.059354	4.816111
290.268111	8000.299021	12.749325	-0.059293	4.816100
290.405609	8000.362442	12.754330	-0.059318	4.816118
290.606967	8000.279553	12.759335	-0.059356	4.816093
290.310079	8000.332926	12.764339	-0.059301	4.816110
290.328251	8000.281967	12.769344	-0.059304	4.816095
290.380830	8000.265830	12.774349	-0.059314	4.816090
290.414410	8000.318810	12.779354	-0.059320	4.816105
290.316976	8000.288186	12.784359	-0.059302	4.816097
290.432428	8000.325559	12.789363	-0.059324	4.816107
290.393959	8000.304558	12.794368	-0.059317	4.816101
290.386994	8000.302298	12.799373	-0.059315	4.816100
290.320038	8000.321388	12.804378	-0.059303	4.816106
290.512897	8000.278952	12.809383	-0.059339	4.816093
290.683518	8000.302368	12.814387	-0.059371	4.816099
290.393064	8000.261818	12.819392	-0.059317	4.816089
290.441422	8000.291556	12.824397	-0.059326	4.816097
290.683347	8000.362223	12.829402	-0.059371	4.816116
290.381744	8000.280860	12.834407	-0.059315	4.816094
290.493551	8000.319235	12.839411	-0.059336	4.816105
290.499395	8000.332170	12.844416	-0.059337	4.816109
290.439719	8000.337499	12.849421	-0.059326	4.816110
290.264563	8000.356755	12.854426	-0.059293	4.816117
290.263114	8000.335360	12.859431	-0.059293	4.816111
290.475901	8000.325347	12.864435	-0.059333	4.816107
290.450186	8000.313128	12.869440	-0.059328	4.816103
290.513473	8000.321766	12.874445	-0.059340	4.816105
290.596347	8000.317936	12.879450	-0.059355	4.816104
290.504964	8000.294903	12.884455	-0.059338	4.816098
290.362005	8000.329707	12.889459	-0.059312	4.816109
290.640744	8000.361504	12.894464	-0.059364	4.816116
290.706070	8000.311403	12.899469	-0.059376	4.816101
290.536049	8000.315791	12.904474	-0.059344	4.816104
290.691854	8000.283368	12.909479	-0.059373	4.816093
290.659647	8000.337287	12.914483	-0.059367	4.816109
290.448044	8000.253289	12.919488	-0.059328	4.816086
290.410361	8000.262225	12.924493	-0.059321	4.816089
290.557522	8000.334371	12.929498	-0.059348	4.816109
290.528473	8000.301787	12.934503	-0.059343	4.816099
290.666072	8000.358799	12.939507	-0.059369	4.816115
290.587346	8000.312486	12.944512	-0.059354	4.816102
290.580104	8000.292054	12.949517	-0.059353	4.816096
290.438233	8000.322603	12.954522	-0.059326	4.816106
290.421342	8000.259249	12.959527	-0.059323	4.816088
290.629253	8000.302580	12.964531	-0.059362	4.816099
290.579561	8000.277101	12.969536	-0.059353	4.816092
290.651631	8000.321164	12.974541	-0.059366	4.816104
290.799245	8000.361260	12.979546	-0.059394	4.816115
290.441169	8000.261770	12.984551	-0.059327	4.816088
290.382600	8000.302385	12.989555	-0.059316	4.816100
290.572319	8000.296226	12.994560	-0.059352	4.816098
290.574436	8000.341153	12.999565	-0.059352	4.816111
290.549032	8000.389852	13.004570	-0.059347	4.816125
290.550929	8000.318291	13.009575	-0.059348	4.816104
290.518968	8000.413893	13.014579	-0.059342	4.816132
290.436919	8000.381412	13.019584	-0.059327	4.816123
290.512566	8000.309057	13.024589	-0.059341	4.816102
290.727427	8000.387780	13.029594	-0.059381	4.816123
290.568184	8000.351756	13.034599	-0.059351	4.816114
290.590458	8000.371402	13.039603	-0.059355	4.816119
290.431409	8000.332175	13.044608	-0.059326	4.816109
290.646629	8000.338237	13.049613	-0.059366	4.816109
290.769711	8000.358650	13.054618	-0.059389	4.816115
290.613941	8000.288492	13.059623	-0.059360	4.816095
290.721365	8000.336405	13.064627	-0.059380	4.816109
290.566243	8000.365644	13.069632	-0.059351	4.816118
290.664985	8000.326838	13.074637	-0.059370	4.816106
290.813433	8000.375498	13.079642	-0.059397	4.816119
290.695330	8000.262211	13.084647	-0.059375	4.816087
290.647700	8000.313712	13.089651	-0.059367	4.816102
290.484366	8000.338527	13.094656	-0.059336	4.816110
290.596543	8000.308515	13.099661	-0.059357	4.816101
290.714061	8000.332032	13.104666	-0.059379	4.816107
290.695243	8000.287879	13.109671	-0.059376	4.816094
290.790153	8000.288544	13.114675	-0.059393	4.816094
290.611397	8000.266057	13.119680	-0.059360	4.816089
290.558011	8000.285393	13.124685	-0.059350	4.816094
290.754429	8000.296455	13.129690	-0.059387	4.816097
290.687185	8000.270656	13.134695	-0.059374	4.816089
290.790930	8000.306747	13.139699	-0.059394	4.816099
290.603036	8000.290505	13.144704	-0.059359	4.816096
290.641918	8000.280531	13.149709	-0.059366	4.816093
290.657894	8000.340671	13.154714	-0.059369	4.816110
290.678401	8000.288685	13.159719	-0.059373	4.816095
290.670332	8000.324877	13.164723	-0.059371	4.816105
290.581621	8000.331814	13.169728	-0.059355	4.816108
290.444660	8000.306883	13.174733	-0.059329	4.816101
290.590489	8000.340534	13.179738	-0.059357	4.816110
290.547245	8000.246778	13.184743	-0.059349	4.816083
290.578515	8000.263382	13.189747	-0.059354	4.816088
290.493061	8000.268242	13.194752	-0.059339	4.816090
290.672283	8000.312119	13.199757	-0.059372	4.816102
290.617246	8000.376309	13.204762	-0.059362	4.816121
290.419625	8000.317144	13.209767	-0.059325	4.816104
290.581666	8000.352159	13.214771	-0.059355	4.816114
290.507906	8000.271740	13.219776	-0.059342	4.816091
290.628118	8000.266453	13.224781	-0.059364	4.816089
290.555182	8000.332454	13.229786	-0.059351	4.816108
290.564271	8000.286672	13.234791	-0.059352	4.816095
290.557815	8000.363502	13.239795	-0.059351	4.816117
290.581148	8000.379961	13.244800	-0.059356	4.816122
290.622754	8000.302711	13.249805	-0.059363	4.816099
290.689989	8000.321039	13.254810	-0.059376	4.816104
290.616162	8000.259854	13.259815	-0.059362	4.816087
290.813946	8000.299795	13.264819	-0.059399	4.816097
290.735172	8000.274854	13.269824	-0.059384	4.816090
290.548726	8000.271463	13.274829	-0.059350	4.816090
290.709363	8000.363091	13.279834	-0.059380	4.816116
290.756984	8000.326560	13.284839	-0.059389	4.816105
290.868218	8000.341414	13.289843	-0.059409	4.816109
290.777460	8000.364345	13.294848	-0.059393	4.816116
290.833120	8000.299106	13.299853	-0.059403	4.816097
290.676530	8000.328318	13.304858	-0.059374	4.816106
290.525374	8000.257176	13.309863	-0.059346	4.816086
290.779710	8000.345167	13.314867	-0.059393	4.816111
290.709767	8000.311838	13.319872	-0.059380	4.816101
290.643620	8000.294608	13.324877	-0.059368	4.816097
290.643316	8000.350177	13.329882	-0.059368	4.816113
290.856346	8000.293148	13.334887	-0.059408	4.816095
290.799794	8000.333800	13.339891	-0.059397	4.816107
290.572092	8000.336069	13.344896	-0.059355	4.816109
290.780096	8000.292841	13.349901	-0.059393	4.816095
290.846103	8000.332519	13.354906	-0.059406	4.816107
290.734872	8000.314468	13.359911	-0.059385	4.816102
290.758848	8000.326664	13.364915	-0.059390	4.816105
290.867137	8000.314748	13.369920	-0.059410	4.816101
290.749809	8000.354293	13.374925	-0.059388	4.816114
290.696269	8000.350116	13.379930	-0.059378	4.816113
290.847049	8000.361417	13.384935	-0.059406	4.816115
290.830720	8000.347231	13.389939	-0.059403	4.816111
290.828709	8000.388876	13.394944	-0.059403	4.816123
290.840100	8000.329243	13.399949	-0.059405	4.816106
290.768785	8000.411304	13.404954	-0.059392	4.816130
290.713501	8000.314122	13.409959	-0.059382	4.816102
290.706038	8000.341776	13.414963	-0.059380	4.816110
290.716415	8000.369754	13.419968	-0.059382	4.816118
290.716208	8000.330214	13.424973	-0.059382	4.816107
290.631079	8000.309433	13.429978	-0.059366	4.816101
290.762975	8000.304359	13.434983	-0.059391	4.816099
290.941699	8000.295863	13.439987	-0.059424	4.816095
290.702081	8000.394094	13.444992	-0.059380	4.816125
290.709250	8000.320492	13.449997	-0.059381	4.816104
290.991698	8000.348083	13.455002	-0.059434	4.816110
290.663146	8000.256610	13.460007	-0.059373	4.816085
290.792440	8000.283548	13.465011	-0.059397	4.816093
290.770962	8000.310947	13.470016	-0.059393	4.816101
290.830263	8000.335542	13.475021	-0.059404	4.816108
291.038941	8000.346828	13.480026	-0.059443	4.816110
290.955459	8000.319664	13.485031	-0.059427	4.816102
290.847853	8000.320914	13.490035	-0.059407	4.816103
290.796080	8000.321044	13.495040	-0.059398	4.816104
290.721860	8000.297255	13.500045	-0.059384	4.816097
290.904716	8000.335856	13.505050	-0.059418	4.816107
290.674155	8000.346621	13.510055	-0.059375	4.816112
290.721431	8000.341075	13.515059	-0.059384	4.816110
290.589137	8000.300198	13.520064	-0.059359	4.816099
290.671259	8000.279257	13.525069	-0.059375	4.816092
290.518423	8000.306400	13.530074	-0.059346	4.816101
290.592323	8000.299201	13.535079	-0.059360	4.816098
290.689224	8000.284940	13.540083	-0.059378	4.816094
290.676143	8000.360581	13.545088	-0.059376	4.816116
290.709176	8000.337676	13.550093	-0.059382	4.816109
290.938321	8000.384601	13.555098	-0.059425	4.816121
290.757290	8000.353523	13.560103	-0.059391	4.816113
290.739487	8000.304045	13.565107	-0.059388	4.816099
290.727578	8000.329480	13.570112	-0.059386	4.816106
290.756651	8000.292611	13.575117	-0.059391	4.816095
290.754072	8000.332109	13.580122	-0.059391	4.816107
290.662360	8000.253499	13.585127	-0.059374	4.816084
290.680768	8000.367116	13.590131	-0.059377	4.816118
290.739706	8000.375675	13.595136	-0.059388	4.816120
290.627883	8000.324484	13.600141	-0.059367	4.816105
290.822437	8000.351543	13.605146	-0.059404	4.816112
290.817826	8000.380317	13.610151	-0.059403	4.816121
290.884765	8000.445661	13.615155	-0.059415	4.816139
290.931364	8000.453995	13.620160	-0.059424	4.816142
290.694238	8000.341745	13.625165	-0.059380	4.816110
290.615052	8000.404426	13.630170	-0.059365	4.816129
290.780285	8000.373243	13.635175	-0.059396	4.816119
290.885737	8000.340971	13.640179	-0.059416	4.816109
290.787158	8000.368034	13.645184	-0.059397	4.816117
290.494641	8000.340268	13.650189	-0.059343	4.816111
290.770592	8000.360260	13.655194	-0.059394	4.816115
290.768762	8000.350613	13.660199	-0.059394	4.816112
290.689718	8000.350247	13.665203	-0.059380	4.816113
290.628241	8000.383328	13.670208	-0.059368	4.816123
290.673242	8000.271943	13.675213	-0.059376	4.816090
290.752232	8000.397351	13.680218	-0.059391	4.816126
290.814515	8000.348263	13.685223	-0.059403	4.816111
290.887798	8000.345327	13.690227	-0.059417	4.816110
290.808469	8000.343887	13.695232	-0.059402	4.816110
290.746906	8000.259415	13.700237	-0.059390	4.816086
290.997215	8000.390080	13.705242	-0.059437	4.816123
290.993415	8000.344063	13.710247	-0.059436	4.816109
290.897841	8000.365837	13.715251	-0.059419	4.816116
290.867542	8000.398418	13.720256	-0.059413	4.816126
291.027176	8000.350034	13.725261	-0.059443	4.816111
290.960673	8000.434321	13.730266	-0.059431	4.816136
290.788392	8000.358517	13.735271	-0.059399	4.816114
290.836604	8000.370086	13.740275	-0.059408	4.816118
290.947430	8000.396689	13.745280	-0.059428	4.816125
290.734817	8000.369310	13.750285	-0.059389	4.816118
290.828140	8000.396662	13.755290	-0.059406	4.816125
290.864983	8000.295815	13.760295	-0.059413	4.816096
290.802615	8000.328880	13.765299	-0.059401	4.816106
290.837968	8000.354108	13.770304	-0.059408	4.816113
291.016857	8000.291114	13.775309	-0.059441	4.816094
291.074698	8000.298584	13.780314	-0.059452	4.816095
290.777103	8000.314540	13.785319	-0.059397	4.816102
290.765707	8000.343191	13.790323	-0.059395	4.816110
290.835378	8000.413928	13.795328	-0.059408	4.816130
290.821025	8000.381611	13.800333	-0.059405	4.816121
290.777422	8000.375477	13.805338	-0.059397	4.816119
290.778933	8000.309252	13.810343	-0.059397	4.816100
290.815809	8000.325958	13.815347	-0.059404	4.816105
290.851054	8000.359733	13.820352	-0.059411	4.816114
290.969503	8000.311668	13.825357	-0.059433	4.816100
290.930848	8000.396461	13.830362	-0.059426	4.816125
290.681750	8000.291474	13.835367	-0.059380	4.816095
290.798837	8000.318190	13.840371	-0.059401	4.816103
290.748235	8000.342921	13.845376	-0.059392	4.816110
290.716794	8000.267547	13.850381	-0.059386	4.816088
290.726333	8000.288029	13.855386	-0.059388	4.816094
290.630535	8000.254229	13.860391	-0.059370	4.816085
290.778597	8000.285784	13.865395	-0.059398	4.816093
290.887320	8000.284563	13.870400	-0.059418	4.816092
290.878165	8000.286538	13.875405	-0.059416	4.816093
290.820528	8000.330376	13.880410	-0.059406	4.816106
290.721897	8000.327515	13.885415	-0.059387	4.816106
291.001729	8000.324067	13.890419	-0.059440	4.816103
290.927988	8000.320591	13.895424	-0.059426	4.816103
290.977985	8000.293721	13.900429	-0.059435	4.816094
291.135647	8000.329726	13.905434	-0.059465	4.816104
290.854619	8000.253011	13.910439	-0.059412	4.816083
290.922408	8000.285241	13.915443	-0.059425	4.816092
290.911989	8000.364137	13.920448	-0.059423	4.816115
290.815936	8000.305752	13.925453	-0.059405	4.816099
291.005243	8000.357295	13.930458	-0.059441	4.816113
290.647980	8000.340105	13.935463	-0.059374	4.816110
290.971837	8000.370588	13.940467	-0.059435	4.816117
291.031299	8000.311830	13.945472	-0.059446	4.816099
290.764088	8000.299487	13.950477	-0.059396	4.816097
290.787043	8000.378990	13.955482	-0.059400	4.816120
290.818081	8000.342157	13.960487	-0.059406	4.816109
291.070294	8000.362785	13.965491	-0.059453	4.816114
291.025748	8000.409000	13.970496	-0.059445	4.816128
290.900950	8000.322306	13.975501	-0.059422	4.816103
290.831434	8000.391576	13.980506	-0.059409	4.816124
290.958674	8000.346877	13.985511	-0.059432	4.816110
290.938869	8000.352932	13.990515	-0.059429	4.816112
290.966790	8000.375887	13.995520	-0.059434	4.816118
290.866474	8000.315288	14.000525	-0.059415	4.816101
290.747275	8000.365485	14.005530	-0.059393	4.816117
290.877075	8000.382815	14.010535	-0.059418	4.816121
290.954537	8000.285914	14.015539	-0.059432	4.816092
290.838706	8000.294495	14.020544	-0.059410	4.816095
290.923511	8000.292838	14.025549	-0.059426	4.816094
291.261024	8000.343875	14.030554	-0.059489	4.816108
290.907485	8000.325684	14.035559	-0.059423	4.816104
290.852486	8000.364227	14.040563	-0.059413	4.816116
291.018800	8000.398252	14.045568	-0.059444	4.816125
290.806119	8000.300340	14.050573	-0.059405	4.816097
290.857416	8000.381428	14.055578	-0.059414	4.816121
290.774918	8000.364968	14.060583	-0.059399	4.816116
290.828395	8000.361672	14.065587	-0.059409	4.816115
290.819682	8000.394647	14.070592	-0.059407	4.816125
290.794851	8000.354658	14.075597	-0.059403	4.816113
290.940369	8000.424639	14.080602	-0.059430	4.816133
290.860778	8000.385790	14.085607	-0.059415	4.816122
290.766439	8000.346673	14.090611	-0.059398	4.816111
290.803514	8000.411473	14.095616	-0.059405	4.816130
290.680823	8000.291689	14.100621	-0.059382	4.816095
290.756823	8000.350786	14.105626	-0.059396	4.816112
290.924533	8000.300412	14.110631	-0.059427	4.816097
291.190540	8000.354421	14.115635	-0.059477	4.816111
290.894977	8000.381101	14.120640	-0.059422	4.816120
290.807742	8000.296160	14.125645	-0.059406	4.816096
291.071350	8000.354400	14.130650	-0.059455	4.816112
290.882535	8000.316767	14.135655	-0.059420	4.816102
290.918734	8000.317431	14.140659	-0.059426	4.816102
290.964308	8000.379180	14.145664	-0.059435	4.816119
290.940345	8000.285774	14.150669	-0.059430	4.816092
290.875043	8000.326266	14.155674	-0.059418	4.816104
290.881666	8000.303949	14.160679	-0.059420	4.816098
291.049810	8000.301673	14.165683	-0.059451	4.816096
291.059405	8000.380934	14.170688	-0.059453	4.816119
290.825835	8000.293328	14.175693	-0.059409	4.816095
291.019315	8000.350290	14.180698	-0.059445	4.816111
291.024912	8000.254216	14.185703	-0.059447	4.816083
290.831064	8000.254964	14.190707	-0.059410	4.816084
291.013272	8000.283935	14.195712	-0.059444	4.816091
290.946245	8000.300886	14.200717	-0.059432	4.816097
290.910920	8000.339788	14.205722	-0.059426	4.816108
290.992379	8000.276087	14.210727	-0.059441	4.816089
291.014095	8000.290380	14.215731	-0.059445	4.816093
290.912010	8000.346233	14.220736	-0.059426	4.816110
290.778309	8000.258309	14.225741	-0.059401	4.816085
291.030791	8000.291766	14.230746	-0.059448	4.816094
291.017348	8000.261603	14.235751	-0.059446	4.816085
290.892602	8000.302081	14.240755	-0.059422	4.816097
291.003802	8000.341515	14.245760	-0.059443	4.816108
291.203981	8000.296007	14.250765	-0.059480	4.816094
291.131030	8000.366283	14.255770	-0.059467	4.816115
291.088778	8000.325977	14.260775	-0.059459	4.816103
291.143595	8000.276753	14.265779	-0.059469	4.816089
291.125942	8000.319182	14.270784	-0.059466	4.816101
291.046733	8000.313469	14.275789	-0.059451	4.816100
290.987252	7999.357032	14.280794	-0.059440	4.815821

291.098261	7996.142872	14.285799	-0.059458	4.814881
291.115358	7990.665367	14.290803	-0.059458	4.813280
291.010080	7983.923415	14.295808	-0.059434	4.811309
290.841067	7976.603686	14.300813	-0.059398	4.809169
290.915318	7969.040869	14.305818	-0.059407	4.806956
290.593785	7961.210285	14.310823	-0.059342	4.804665
290.626509	7953.408792	14.315827	-0.059343	4.802379
290.832778	7945.417962	14.320832	-0.059376	4.800037
290.637250	7937.455133	14.325837	-0.059335	4.797703
290.593042	7929.410442	14.330842	-0.059321	4.795343
290.404600	7921.406736	14.335847	-0.059281	4.792995
290.380711	7913.335272	14.340851	-0.059271	4.790625
290.533464	7905.424685	14.345856	-0.059295	4.788301
290.456465	7897.362425	14.350861	-0.059275	4.785932
290.445385	7889.455938	14.355866	-0.059268	4.783607
290.412343	7881.409751	14.360871	-0.059257	4.781239
290.551381	7873.443336	14.365875	-0.059277	4.778894
290.351382	7865.463011	14.370880	-0.059235	4.776545
290.128885	7857.405858	14.375885	-0.059188	4.774172
290.434773	7849.403892	14.380890	-0.059240	4.771811
290.210990	7841.339981	14.385895	-0.059193	4.769434
290.150665	7833.446444	14.390899	-0.059177	4.767105
290.116722	7825.358409	14.395904	-0.059165	4.764717
290.023908	7817.405725	14.400909	-0.059143	4.762369
290.093917	7809.430699	14.405914	-0.059151	4.760011
290.000953	7801.423648	14.410919	-0.059128	4.757644
289.839133	7793.433436	14.415923	-0.059093	4.755281
289.740283	7785.334190	14.420928	-0.059069	4.752885
289.692362	7777.272401	14.425933	-0.059055	4.750497
289.830005	7769.360303	14.430938	-0.059076	4.748153
289.803310	7761.319463	14.435943	-0.059066	4.745769
289.822858	7753.360074	14.440947	-0.059064	4.743409
289.622117	7745.367294	14.445952	-0.059022	4.741038
289.492808	7737.362617	14.450957	-0.058992	4.738662
289.568697	7729.399073	14.455962	-0.059001	4.736297
289.489620	7721.324282	14.460967	-0.058981	4.733897
289.438881	7713.311681	14.465971	-0.058967	4.731515
289.494315	7705.286475	14.470976	-0.058972	4.729128
289.260796	7697.294694	14.475981	-0.058923	4.726750
289.419942	7689.301770	14.480986	-0.058948	4.724370
289.153454	7681.328290	14.485991	-0.058893	4.721995
289.102942	7673.318209	14.490995	-0.058878	4.719608
289.123458	7665.389325	14.496000	-0.058877	4.717243
289.130867	7657.305282	14.501005	-0.058873	4.714831
289.165437	7649.328108	14.506010	-0.058874	4.712450
288.825732	7641.255284	14.511015	-0.058806	4.710039
289.031713	7633.286828	14.516019	-0.058839	4.707658
289.148469	7625.353889	14.521024	-0.058856	4.705286
288.835118	7617.318847	14.526029	-0.058792	4.702883
288.895278	7609.350722	14.531034	-0.058798	4.700498
289.102008	7601.348258	14.536039	-0.058832	4.698101
289.072802	7593.268675	14.541043	-0.058821	4.695681
288.858765	7585.302162	14.546048	-0.058776	4.693293
288.934821	7577.291084	14.551053	-0.058785	4.690891
288.878467	7569.325720	14.556058	-0.058769	4.688501
288.658055	7561.264448	14.561063	-0.058723	4.686081
288.685570	7553.319393	14.566067	-0.058723	4.683695
288.717245	7545.316097	14.571072	-0.058724	4.681289
288.345426	7537.271564	14.576077	-0.058649	4.678872
288.257645	7529.355676	14.581082	-0.058628	4.676490
288.328698	7521.246831	14.586087	-0.058636	4.674050
288.255265	7513.116415	14.591091	-0.058617	4.671601
288.229870	7505.220564	14.596096	-0.058607	4.669222
288.125463	7497.226820	14.601101	-0.058583	4.666813
288.248929	7489.203374	14.606106	-0.058600	4.664393
288.152564	7481.269719	14.611111	-0.058577	4.661999
288.346412	7473.242492	14.616115	-0.058608	4.659575
288.277658	7465.324447	14.621120	-0.058590	4.657183
288.012380	7457.199894	14.626125	-0.058536	4.654728
287.936562	7449.211724	14.631130	-0.058516	4.652312
287.871571	7441.244295	14.636135	-0.058499	4.649902
287.782045	7433.212873	14.641139	-0.058477	4.647471
287.640767	7425.229795	14.646144	-0.058446	4.645053
287.638686	7417.229859	14.651149	-0.058440	4.642629
287.695068	7409.233302	14.656154	-0.058446	4.640204
287.589010	7401.277371	14.661159	-0.058421	4.637791
287.621863	7393.206809	14.666163	-0.058422	4.635341
287.738116	7385.223002	14.671168	-0.058438	4.632917
287.445717	7377.159931	14.676173	-0.058378	4.630467
287.360399	7369.236331	14.681178	-0.058357	4.628059
287.397717	7361.200230	14.686183	-0.058359	4.625615
287.617753	7353.205734	14.691187	-0.058395	4.623182
287.414939	7345.206233	14.696192	-0.058352	4.620746
287.413256	7337.212467	14.701197	-0.058347	4.618311
287.362101	7329.206452	14.706202	-0.058332	4.615871
287.211264	7321.192254	14.711207	-0.058299	4.613427
287.305013	7313.111116	14.716211	-0.058311	4.610961
287.407643	7305.194798	14.721216	-0.058325	4.608544
287.289565	7297.147487	14.726221	-0.058298	4.606086
287.140541	7289.184162	14.731226	-0.058265	4.603653
287.093688	7281.169038	14.736231	-0.058251	4.601202
286.959667	7273.185718	14.741235	-0.058221	4.598760
286.850196	7265.201607	14.746240	-0.058195	4.596316
286.763118	7257.114788	14.751245	-0.058174	4.593839
286.871815	7249.134204	14.756250	-0.058189	4.591394
286.816557	7241.125314	14.761255	-0.058173	4.588938
286.662627	7233.111636	14.766259	-0.058140	4.586480
286.686142	7225.126601	14.771264	-0.058139	4.584029
286.673469	7217.159082	14.776269	-0.058131	4.581582
286.579984	7209.151225	14.781274	-0.058109	4.579122
286.566421	7201.176041	14.786279	-0.058101	4.576670
286.656786	7193.141059	14.791283	-0.058113	4.574199
286.687953	7185.148019	14.796288	-0.058113	4.571739
286.493219	7177.108007	14.801293	-0.058072	4.569263
286.549792	7169.169171	14.806298	-0.058077	4.566818
286.462714	7161.112384	14.811303	-0.058056	4.564334
286.416116	7153.159099	14.816307	-0.058042	4.561881
286.418303	7145.167507	14.821312	-0.058037	4.559415
286.052433	7137.144909	14.826317	-0.057964	4.556938
286.059135	7129.135789	14.831322	-0.057960	4.554463
285.997260	7121.093888	14.836327	-0.057943	4.551978
285.950145	7113.093703	14.841331	-0.057929	4.549504
285.800756	7105.159800	14.846336	-0.057896	4.547048
285.844943	7097.099455	14.851341	-0.057899	4.544553
285.995148	7089.176101	14.856346	-0.057922	4.542099
285.857876	7081.111169	14.861351	-0.057891	4.539599
285.675780	7073.135484	14.866355	-0.057852	4.537125
285.723782	7065.122927	14.871360	-0.057856	4.534639
285.697633	7057.143262	14.876365	-0.057846	4.532162
285.933049	7049.118435	14.881370	-0.057885	4.529670
285.678421	7041.154724	14.886375	-0.057832	4.527194
285.647446	7033.086872	14.891379	-0.057821	4.524685
285.636958	7025.175879	14.896384	-0.057814	4.522224
285.407852	7017.075968	14.901389	-0.057766	4.519702
285.538840	7009.163896	14.906394	-0.057786	4.517238
285.480952	7001.098030	14.911399	-0.057770	4.514724
285.321184	6993.008311	14.916403	-0.057735	4.512201
285.329375	6985.045128	14.921408	-0.057731	4.509717
285.142647	6977.075662	14.926413	-0.057691	4.507228
285.255117	6969.057630	14.931418	-0.057707	4.504724
285.145749	6961.126505	14.936423	-0.057681	4.502245
285.263551	6953.074357	14.941427	-0.057698	4.499728
285.291937	6945.135092	14.946432	-0.057698	4.497244
285.070797	6937.049599	14.951437	-0.057652	4.494712
285.069527	6929.072635	14.956442	-0.057646	4.492214
284.974020	6921.036151	14.961447	-0.057623	4.489695
284.851490	6913.063174	14.966451	-0.057595	4.487195
284.801767	6905.067217	14.971456	-0.057581	4.484686
284.722060	6897.104857	14.976461	-0.057561	4.482186
284.652000	6889.043550	14.981466	-0.057543	4.479654
284.762384	6881.112310	14.986471	-0.057558	4.477161
284.730254	6873.015067	14.991475	-0.057547	4.474615
284.750277	6865.040004	14.996480	-0.057546	4.472106
284.469262	6857.002940	15.001485	-0.057488	4.469575
284.652655	6849.043236	15.006490	-0.057517	4.467068
284.554903	6841.004617	15.011495	-0.057494	4.464534
284.430360	6833.067880	15.016499	-0.057465	4.462031
284.489621	6825.087235	15.021504	-0.057471	4.459513
284.394000	6817.053419	15.026509	-0.057448	4.456977
284.451812	6809.060100	15.031514	-0.057454	4.454452
284.129057	6801.032063	15.036519	-0.057389	4.451913
284.310002	6792.948783	15.041523	-0.057417	4.449358
284.336223	6785.013895	15.046528	-0.057417	4.446847
284.170711	6776.963481	15.051533	-0.057381	4.444298
284.121314	6769.083874	15.056538	-0.057367	4.441801
284.063710	6761.011888	15.061543	-0.057351	4.439242
283.904642	6753.036368	15.066547	-0.057316	4.436712
283.810852	6745.018430	15.071552	-0.057293	4.434168
283.850448	6736.974948	15.076557	-0.057295	4.431614
283.876312	6729.000127	15.081562	-0.057295	4.429080
283.715913	6720.978293	15.086567	-0.057260	4.426530
283.718916	6713.045346	15.091571	-0.057255	4.424006
283.656847	6705.013850	15.096576	-0.057239	4.421450
283.523556	6696.956637	15.101581	-0.057209	4.418884
283.794640	6688.958334	15.106586	-0.057254	4.416337
283.752399	6680.950334	15.111591	-0.057241	4.413783
283.635761	6672.970552	15.116595	-0.057214	4.411237
283.488607	6665.019341	15.121600	-0.057181	4.408699
283.401654	6656.956576	15.126605	-0.057160	4.406124
283.342201	6649.030995	15.131610	-0.057144	4.403591
283.087787	6640.976266	15.136615	-0.057091	4.401014
283.257225	6633.006757	15.141619	-0.057118	4.398465
283.281987	6625.009906	15.146624	-0.057117	4.395906
282.987136	6616.943758	15.151629	-0.057057	4.393321
283.247702	6608.956506	15.156634	-0.057100	4.390762
283.156823	6600.990128	15.161639	-0.057078	4.388207
282.999018	6592.960453	15.166643	-0.057044	4.385630
282.863676	6585.017834	15.171648	-0.057013	4.383079
283.015918	6576.983814	15.176653	-0.057037	4.380499
282.963693	6569.014215	15.181658	-0.057022	4.377937
282.817295	6560.974241	15.186663	-0.056989	4.375351
282.873458	6553.010297	15.191667	-0.056995	4.372788
282.818015	6544.956981	15.196672	-0.056979	4.370195
282.713580	6537.001363	15.201677	-0.056954	4.367631
282.664637	6529.006883	15.206682	-0.056940	4.365053
282.628535	6521.026599	15.211687	-0.056928	4.362479
282.417305	6512.969125	15.216691	-0.056884	4.359877
282.559282	6505.038621	15.221696	-0.056905	4.357317
282.438335	6496.972717	15.226701	-0.056877	4.354710
282.488915	6488.874709	15.231706	-0.056882	4.352091
282.266014	6480.925643	15.236711	-0.056835	4.349518
282.278879	6472.937349	15.241715	-0.056832	4.346932
282.260697	6464.971754	15.246720	-0.056824	4.344352
282.165053	6456.959452	15.251725	-0.056801	4.341755
282.103917	6448.990771	15.256730	-0.056784	4.339170
282.293897	6440.975715	15.261735	-0.056814	4.336570
282.029662	6432.927410	15.266739	-0.056760	4.333955
281.964747	6424.953047	15.271744	-0.056743	4.331364
281.947374	6416.958517	15.276749	-0.056734	4.328765
282.004166	6408.934649	15.281754	-0.056740	4.326155
282.148086	6400.957901	15.286759	-0.056761	4.323560
281.868397	6392.953597	15.291763	-0.056704	4.320951
281.794684	6384.992973	15.296768	-0.056685	4.318356
281.839754	6376.964752	15.301773	-0.056688	4.315739
281.816155	6368.960096	15.306778	-0.056679	4.313127
281.668525	6360.890356	15.311783	-0.056646	4.310491
281.575606	6352.938109	15.316787	-0.056624	4.307893
281.727416	6344.937527	15.321792	-0.056647	4.305279
281.559471	6336.946053	15.326797	-0.056610	4.302664
281.502373	6328.938889	15.331802	-0.056594	4.300043
281.341099	6320.972370	15.336807	-0.056559	4.297433
281.368394	6312.880698	15.341811	-0.056559	4.294782
281.473722	6304.949276	15.346816	-0.056574	4.292182
281.396215	6296.882297	15.351821	-0.056554	4.289535
281.407720	6288.945637	15.356826	-0.056551	4.286930
281.298388	6280.877005	15.361831	-0.056525	4.284278
281.263173	6272.935087	15.366835	-0.056514	4.281668
281.104540	6265.007660	15.371840	-0.056479	4.279059
280.915988	6256.937917	15.376845	-0.056439	4.276402
281.040368	6248.930040	15.381850	-0.056457	4.273766
280.814354	6240.875112	15.386855	-0.056409	4.271110
280.720014	6232.849461	15.391859	-0.056387	4.268464
280.821642	6224.867425	15.396864	-0.056400	4.265831
280.735103	6216.918687	15.401869	-0.056379	4.263206
280.842698	6208.893396	15.406874	-0.056394	4.260557
280.731198	6200.950464	15.411879	-0.056368	4.257930
280.835645	6192.888926	15.416883	-0.056382	4.255265
280.757418	6184.922997	15.421888	-0.056363	4.252628
280.571471	6176.887597	15.426893	-0.056323	4.249966
280.599141	6168.943019	15.431898	-0.056323	4.247334
280.654697	6160.935783	15.436903	-0.056328	4.244679
280.547816	6152.930384	15.441907	-0.056303	4.242022
280.615181	6144.984561	15.446912	-0.056310	4.239385
280.378784	6136.954236	15.451917	-0.056261	4.236716
280.241994	6128.938547	15.456922	-0.056231	4.234050
280.222220	6120.926606	15.461927	-0.056222	4.231385
280.244375	6112.881049	15.466931	-0.056221	4.228708
280.161859	6104.897881	15.471936	-0.056200	4.226048
280.023285	6096.927920	15.476941	-0.056169	4.223391
280.053759	6088.923595	15.481946	-0.056170	4.220723
280.005104	6080.959336	15.486951	-0.056155	4.218065
279.733824	6072.932696	15.491955	-0.056100	4.215382
279.897407	6064.929481	15.496960	-0.056125	4.212710
279.916942	6056.884149	15.501965	-0.056123	4.210021
279.988934	6048.941313	15.506970	-0.056132	4.207365
279.861749	6040.898415	15.511975	-0.056103	4.204671
279.696521	6032.991389	15.516979	-0.056067	4.202021
279.930200	6024.916345	15.521984	-0.056105	4.199318
279.709550	6016.982987	15.526989	-0.056059	4.196655
279.716087	6008.878585	15.531994	-0.056055	4.193935
279.602023	6000.829608	15.536999	-0.056029	4.191231
279.609080	5992.831378	15.542003	-0.056025	4.188544
279.558857	5984.880903	15.547008	-0.056010	4.185870
279.653773	5976.892975	15.552013	-0.056023	4.183184
279.336159	5968.908265	15.557018	-0.055959	4.180492
279.341992	5960.960308	15.562023	-0.055954	4.177815
279.205926	5952.909934	15.567027	-0.055924	4.175099
279.111953	5944.929206	15.572032	-0.055901	4.172406
278.957905	5936.874242	15.577037	-0.055867	4.169686
278.985895	5928.876003	15.582042	-0.055867	4.166985
278.891925	5920.901694	15.587047	-0.055845	4.164289
278.890045	5912.926809	15.592051	-0.055839	4.161592
278.873502	5904.927153	15.597056	-0.055831	4.158884
278.959102	5896.898920	15.602061	-0.055842	4.156166
278.822689	5888.895287	15.607066	-0.055811	4.153453
278.645906	5880.861487	15.612071	-0.055773	4.150727
278.704419	5872.825106	15.617075	-0.055779	4.148001
278.852500	5864.864490	15.622080	-0.055801	4.145299
278.766260	5856.912412	15.627085	-0.055780	4.142597
278.652233	5848.890327	15.632090	-0.055754	4.139868
278.554262	5840.921653	15.637095	-0.055730	4.137156
278.352590	5832.872923	15.642099	-0.055687	4.134414
278.429670	5824.861122	15.647104	-0.055697	4.131685
278.310924	5816.862378	15.652109	-0.055669	4.128957
278.308251	5808.889585	15.657114	-0.055664	4.126238
278.411186	5800.900934	15.662119	-0.055678	4.123512
278.369455	5792.889799	15.667123	-0.055665	4.120775
278.265519	5784.933726	15.672128	-0.055640	4.118055
278.063751	5776.889762	15.677133	-0.055598	4.115301
278.108894	5768.863290	15.682138	-0.055601	4.112555
278.133653	5760.837445	15.687143	-0.055600	4.109807
278.068168	5752.861255	15.692147	-0.055583	4.107072
278.233355	5744.886460	15.697152	-0.055608	4.104340
277.974865	5736.880774	15.702157	-0.055555	4.101589
278.211104	5728.867597	15.707162	-0.055594	4.098841
277.833715	5720.932636	15.712167	-0.055519	4.096109
277.765737	5712.905259	15.717171	-0.055501	4.093348
277.962922	5704.875115	15.722176	-0.055532	4.090588
277.683529	5696.891104	15.727181	-0.055475	4.087835
277.531635	5688.886886	15.732186	-0.055442	4.085075
277.642554	5680.915162	15.737191	-0.055457	4.082328
277.607904	5672.909158	15.742195	-0.055445	4.079565
277.616198	5664.976538	15.747200	-0.055442	4.076827
277.691818	5656.910219	15.752205	-0.055451	4.074041
277.635603	5648.897893	15.757210	-0.055435	4.071270
277.493337	5640.912485	15.762215	-0.055403	4.068506
277.471684	5632.868297	15.767219	-0.055394	4.065720
277.510719	5624.955148	15.772224	-0.055396	4.062980
277.473717	5616.932433	15.777229	-0.055384	4.060198
277.295558	5608.962296	15.782234	-0.055346	4.057431
277.247963	5600.934867	15.787239	-0.055332	4.054643
277.260763	5592.912333	15.792243	-0.055329	4.051857
277.007421	5584.955548	15.797248	-0.055277	4.049087
276.963567	5576.929348	15.802253	-0.055263	4.046294
277.130844	5568.926026	15.807258	-0.055289	4.043511
277.228670	5560.952526	15.812263	-0.055303	4.040735
276.802551	5552.957893	15.817267	-0.055218	4.037942
276.920012	5544.943603	15.822272	-0.055235	4.035148
276.699335	5536.800588	15.827277	-0.055188	4.032302
276.477086	5528.882380	15.832282	-0.055142	4.029533
276.710426	5520.881682	15.837287	-0.055180	4.026740
276.648683	5512.891856	15.842291	-0.055163	4.023944
276.792418	5504.900622	15.847296	-0.055185	4.021149
276.576439	5496.912508	15.852301	-0.055140	4.018347
276.457664	5488.907176	15.857306	-0.055112	4.015540
276.315745	5480.957436	15.862311	-0.055081	4.012749
276.259907	5472.904637	15.867315	-0.055065	4.009921
276.539917	5464.930831	15.872320	-0.055112	4.007125
276.398891	5456.905495	15.877325	-0.055081	4.004301
276.141671	5448.948675	15.882330	-0.055028	4.001498
276.270056	5440.934370	15.887335	-0.055046	3.998679
276.309755	5432.891518	15.892339	-0.055049	3.995847
276.164830	5424.924579	15.897344	-0.055017	3.993036
276.135881	5416.876723	15.902349	-0.055006	3.990196
276.135015	5408.904075	15.907354	-0.055001	3.987382
276.107289	5400.895874	15.912359	-0.054990	3.984552
275.924653	5392.947210	15.917363	-0.054951	3.981740
276.072275	5384.900953	15.922368	-0.054973	3.978895
275.866763	5376.946225	15.927373	-0.054930	3.976076
275.734607	5368.939240	15.932378	-0.054900	3.973237
275.798212	5360.899940	15.937383	-0.054907	3.970388
275.900736	5352.916483	15.942387	-0.054921	3.967557
275.633697	5344.920757	15.947392	-0.054866	3.964714
275.414782	5337.015594	15.952397	-0.054820	3.961902
275.559905	5328.964732	15.957402	-0.054842	3.959042
275.456665	5320.989248	15.962407	-0.054818	3.956202
275.384943	5312.916373	15.967411	-0.054799	3.953326
275.579638	5304.931321	15.972416	-0.054830	3.950485
275.436292	5296.925210	15.977421	-0.054798	3.947627
275.407434	5288.918594	15.982426	-0.054788	3.944770
275.225597	5281.003826	15.987431	-0.054749	3.941940
275.392498	5272.958309	15.992435	-0.054775	3.939068
275.469886	5264.985777	15.997440	-0.054784	3.936218
275.174348	5256.958695	16.002445	-0.054724	3.933340
275.384976	5248.942465	16.007450	-0.054758	3.930473
275.301954	5240.991717	16.012455	-0.054737	3.927622
275.208311	5232.954204	16.017459	-0.054714	3.924738
275.114678	5225.040898	16.022464	-0.054692	3.921896
275.103515	5217.016320	16.027469	-0.054685	3.919013
274.974192	5208.993140	16.032474	-0.054655	3.916127
274.920864	5200.979068	16.037479	-0.054640	3.913243
274.667170	5192.987953	16.042483	-0.054588	3.910362
274.628237	5184.978132	16.047488	-0.054575	3.907475
274.249435	5176.975045	16.052493	-0.054500	3.904583
274.425570	5168.986129	16.057498	-0.054527	3.901704
274.505182	5160.999332	16.062503	-0.054537	3.898822
274.280525	5152.983067	16.067507	-0.054490	3.895921
274.410048	5144.980525	16.072512	-0.054509	3.893030
274.423085	5136.950230	16.077517	-0.054506	3.890124
274.373381	5128.993826	16.082522	-0.054492	3.887242
274.343467	5121.004430	16.087527	-0.054481	3.884346
274.164183	5112.981494	16.092531	-0.054442	3.881433
274.228189	5105.052500	16.097536	-0.054449	3.878556
274.235847	5097.009469	16.102541	-0.054445	3.875635
274.010403	5088.791657	16.107546	-0.054398	3.872644
274.021725	5080.809658	16.112551	-0.054395	3.869740
273.645118	5072.875746	16.117555	-0.054320	3.866844
273.809521	5064.900177	16.122560	-0.054345	3.863942
273.944755	5056.927823	16.127565	-0.054365	3.861038
273.860156	5048.978385	16.132570	-0.054345	3.858136
273.857283	5040.987822	16.137575	-0.054339	3.855218
273.736439	5032.944810	16.142579	-0.054311	3.852276
273.807017	5024.971822	16.147584	-0.054319	3.849362
273.545084	5017.006812	16.152589	-0.054265	3.846442
273.501241	5008.984891	16.157594	-0.054252	3.843503
273.638926	5001.038324	16.162599	-0.054272	3.840593
273.384453	4993.030050	16.167603	-0.054220	3.837650
273.453378	4985.027970	16.172608	-0.054227	3.834713
273.430151	4977.014183	16.177613	-0.054218	3.831769
273.332373	4968.990363	16.182618	-0.054195	3.828817
273.236409	4961.032048	16.187623	-0.054172	3.825886
273.360234	4953.010747	16.192627	-0.054189	3.822935
273.477336	4945.039162	16.197632	-0.054206	3.820000
273.201932	4937.075557	16.202637	-0.054150	3.817057
273.102911	4929.047329	16.207642	-0.054126	3.814092
273.141319	4921.066567	16.212647	-0.054128	3.811145
272.860471	4913.078982	16.217651	-0.054071	3.808186
272.897713	4905.079488	16.222656	-0.054072	3.805227
273.171012	4897.076835	16.227661	-0.054118	3.802270
272.895885	4889.086699	16.232666	-0.054062	3.799303
272.914238	4881.109489	16.237671	-0.054060	3.796346
272.786217	4873.051141	16.242675	-0.054031	3.793352
272.756724	4865.031279	16.247680	-0.054020	3.790373
272.640380	4857.072361	16.252685	-0.053993	3.787412
272.605964	4849.036893	16.257690	-0.053982	3.784422
272.582426	4841.119483	16.262695	-0.053972	3.781474
272.308098	4833.088236	16.267699	-0.053916	3.778476
272.388309	4825.072591	16.272704	-0.053926	3.775488
272.498084	4817.068193	16.277709	-0.053941	3.772504
272.523524	4809.042534	16.282714	-0.053941	3.769507
272.474087	4801.107057	16.287719	-0.053926	3.766540
272.274466	4793.070920	16.292723	-0.053884	3.763529
272.239829	4785.091382	16.297728	-0.053872	3.760541
272.082266	4777.127308	16.302733	-0.053838	3.757554
272.026801	4769.102691	16.307738	-0.053822	3.754544
272.182564	4761.118254	16.312743	-0.053846	3.751551
272.004964	4753.100655	16.317747	-0.053808	3.748536
271.748863	4745.108516	16.322752	-0.053755	3.745526
271.794534	4737.111011	16.327757	-0.053758	3.742518
271.989722	4729.097439	16.332762	-0.053790	3.739506
271.820560	4721.176556	16.337767	-0.053753	3.736517
271.654241	4713.109636	16.342771	-0.053717	3.733472
271.826247	4705.102745	16.347776	-0.053744	3.730454
271.765762	4697.127520	16.352781	-0.053727	3.727440
271.642830	4689.119758	16.357786	-0.053699	3.724410
271.528364	4681.193108	16.362791	-0.053673	3.721409
271.560371	4673.169716	16.367795	-0.053673	3.718372
271.687673	4665.188026	16.372800	-0.053692	3.715350
271.600783	4657.099636	16.377805	-0.053671	3.712281
271.426957	4649.089286	16.382810	-0.053633	3.709236
271.282976	4641.129698	16.387815	-0.053601	3.706209
271.197796	4633.136801	16.392819	-0.053580	3.703168
271.315647	4625.160447	16.397824	-0.053597	3.700136
271.006819	4617.225431	16.402829	-0.053534	3.697107
270.924617	4609.189900	16.407834	-0.053514	3.694042
271.270615	4601.143161	16.412839	-0.053573	3.690981
271.015776	4593.172231	16.417843	-0.053520	3.687932
271.016570	4585.211774	16.422848	-0.053515	3.684891
270.896868	4577.261690	16.427853	-0.053488	3.681848
270.833645	4569.237885	16.432858	-0.053471	3.678775
270.993789	4561.214279	16.437863	-0.053496	3.675706
270.980005	4553.159936	16.442867	-0.053488	3.672618
271.147291	4545.184181	16.447872	-0.053514	3.669562
270.919555	4537.224137	16.452877	-0.053466	3.666500
270.606999	4529.216405	16.457882	-0.053403	3.663414
270.562919	4521.232539	16.462887	-0.053390	3.660342
270.424637	4513.231711	16.467891	-0.053359	3.657259
270.405864	4505.232918	16.472896	-0.053350	3.654176
270.208103	4497.204380	16.477901	-0.053308	3.651075
270.256855	4489.239697	16.482906	-0.053312	3.648003
270.109708	4481.241650	16.487911	-0.053279	3.644909
270.003584	4473.274317	16.492915	-0.053254	3.641826
270.170290	4465.284722	16.497920	-0.053280	3.638739
270.005675	4457.269666	16.502925	-0.053244	3.635631
270.110620	4449.185920	16.507930	-0.053259	3.632501
270.243917	4441.205297	16.512935	-0.053278	3.629408
269.954280	4433.213931	16.517939	-0.053219	3.626298
270.168476	4425.263824	16.522944	-0.053254	3.623214
270.035370	4417.265815	16.527949	-0.053224	3.620100
270.104513	4409.291171	16.532954	-0.053232	3.616998
269.975783	4401.285862	16.537959	-0.053203	3.613875
269.627060	4393.266887	16.542963	-0.053133	3.610739
269.838904	4385.270153	16.547968	-0.053167	3.607624
269.906107	4377.258439	16.552973	-0.053174	3.604496
269.717040	4369.306027	16.557978	-0.053134	3.601382
269.859124	4361.352350	16.562983	-0.053155	3.598274
269.484399	4353.352045	16.567987	-0.053080	3.595130
269.490626	4345.336636	16.572992	-0.053076	3.591989
269.488291	4337.334420	16.577997	-0.053071	3.588849
269.319623	4329.347117	16.583002	-0.053034	3.585708
269.488529	4321.380044	16.588007	-0.053060	3.582582
269.258053	4313.357295	16.593011	-0.053012	3.579419
269.387354	4305.418095	16.598016	-0.053031	3.576297
269.388695	4297.406314	16.603021	-0.053026	3.573141
269.191449	4289.365353	16.608026	-0.052984	3.569964
269.092896	4281.443062	16.613031	-0.052961	3.566833
269.286239	4273.373053	16.618035	-0.052992	3.563651
269.227353	4265.405120	16.623040	-0.052976	3.560498
269.041080	4257.440193	16.628045	-0.052936	3.557340
269.120139	4249.379466	16.633050	-0.052945	3.554149
268.887859	4241.348061	16.638055	-0.052897	3.550958
268.719884	4233.372714	16.643059	-0.052860	3.547788
268.867681	4225.343520	16.648064	-0.052883	3.544603
268.965020	4217.404496	16.653069	-0.052896	3.541449
268.732212	4209.396667	16.658074	-0.052847	3.538256
268.779776	4201.412109	16.663079	-0.052851	3.535077
268.607563	4193.404955	16.668083	-0.052814	3.531879
268.502052	4185.419691	16.673088	-0.052789	3.528690
268.410031	4177.435217	16.678093	-0.052767	3.525498
268.442024	4169.468197	16.683098	-0.052767	3.522315
268.380439	4161.478001	16.688103	-0.052751	3.519116
268.162219	4153.501505	16.693107	-0.052705	3.515915
268.425303	4145.483396	16.698112	-0.052749	3.512709
268.258222	4137.469442	16.703117	-0.052712	3.509488
268.230345	4129.481837	16.708122	-0.052702	3.506280
268.051821	4121.503766	16.713127	-0.052664	3.503068
267.919543	4113.501631	16.718131	-0.052634	3.499844
268.152326	4105.547842	16.723136	-0.052672	3.496649
268.081378	4097.545658	16.728141	-0.052654	3.493421
267.873334	4089.513542	16.733146	-0.052610	3.490174
267.959878	4081.559692	16.738151	-0.052621	3.486965
267.616876	4073.553062	16.743155	-0.052552	3.483718
267.683898	4065.563024	16.748160	-0.052559	3.480488
267.837862	4057.605960	16.753165	-0.052583	3.477271
267.649223	4049.583678	16.758170	-0.052542	3.474013
267.643087	4041.544700	16.763175	-0.052536	3.470752
267.458952	4033.538040	16.768179	-0.052497	3.467494
267.519529	4025.570377	16.773184	-0.052503	3.464258
267.492790	4017.594793	16.778189	-0.052493	3.461012
267.373909	4009.627109	16.783194	-0.052465	3.457764
267.382525	4001.602494	16.788199	-0.052462	3.454493
267.231233	3993.613504	16.793203	-0.052428	3.451229
267.281990	3985.599980	16.798208	-0.052433	3.447958
267.224681	3977.608030	16.803213	-0.052417	3.444689
267.216344	3969.636548	16.808218	-0.052410	3.441427
267.107554	3961.667755	16.813223	-0.052385	3.438160
267.072607	3953.664104	16.818227	-0.052373	3.434878
267.110461	3945.639430	16.823232	-0.052375	3.431586
266.955125	3937.645681	16.828237	-0.052341	3.428298
266.980200	3929.619231	16.833242	-0.052340	3.424999
266.965849	3921.689402	16.838247	-0.052332	3.421735
266.799128	3913.684879	16.843251	-0.052296	3.418432
266.794404	3905.699153	16.848256	-0.052290	3.415140
266.807610	3897.703032	16.853261	-0.052287	3.411840
266.725962	3889.689199	16.858266	-0.052267	3.408527
266.541473	3881.753548	16.863271	-0.052228	3.405239
266.437563	3873.752660	16.868275	-0.052203	3.401924
266.536765	3865.767679	16.873280	-0.052216	3.398619
266.388881	3857.807899	16.878285	-0.052184	3.395312
266.066347	3849.687053	16.883290	-0.052118	3.391930
266.224008	3841.706424	16.888295	-0.052143	3.388619
266.209672	3833.697624	16.893299	-0.052135	3.385287
266.013254	3825.771915	16.898304	-0.052093	3.381981
266.340655	3817.768934	16.903309	-0.052149	3.378657
266.098620	3809.784906	16.908314	-0.052099	3.375317
265.945059	3801.823113	16.913319	-0.052065	3.371987
265.881638	3793.781026	16.918323	-0.052048	3.368623
265.946935	3785.797261	16.923328	-0.052055	3.365285
265.748637	3777.847485	16.928333	-0.052013	3.361948
265.773314	3769.852499	16.933338	-0.052012	3.358597
265.846421	3761.868048	16.938343	-0.052021	3.355248
265.658246	3753.825473	16.943347	-0.051981	3.351863
265.728633	3745.817206	16.948352	-0.051988	3.348498
265.596020	3737.843280	16.953357	-0.051959	3.345136
265.585969	3729.882443	16.958362	-0.051952	3.341781
265.658630	3721.890668	16.963367	-0.051960	3.338413
265.556869	3713.889484	16.968371	-0.051936	3.335031
265.548765	3705.896478	16.973376	-0.051929	3.331652
265.457767	3697.904035	16.978381	-0.051907	3.328267
265.278618	3689.902389	16.983386	-0.051869	3.324872
265.489628	3681.956683	16.988391	-0.051903	3.321511
265.081190	3673.985562	16.993395	-0.051821	3.318113
265.137436	3665.975494	16.998400	-0.051827	3.314712
265.145980	3657.926449	17.003405	-0.051823	3.311290
265.103032	3649.933502	17.008410	-0.051810	3.307885
264.989275	3641.938943	17.013415	-0.051784	3.304474
264.904749	3633.983763	17.018419	-0.051763	3.301078
265.195229	3625.990450	17.023424	-0.051812	3.297675
265.116276	3618.014683	17.028429	-0.051792	3.294263
264.801015	3610.016468	17.033434	-0.051728	3.290828
264.864078	3602.049851	17.038439	-0.051735	3.287418
264.797707	3594.057193	17.043443	-0.051717	3.283988
264.566145	3586.082624	17.048448	-0.051669	3.280556
264.495986	3578.102033	17.053453	-0.051651	3.277124
264.497371	3570.077706	17.058458	-0.051646	3.273673
264.505525	3562.050366	17.063463	-0.051642	3.270216
264.537742	3554.079286	17.068467	-0.051643	3.266781
264.666352	3546.075314	17.073472	-0.051662	3.263333
264.604565	3538.105683	17.078477	-0.051645	3.259887
264.425127	3530.141495	17.083482	-0.051606	3.256436
264.420125	3522.145443	17.088487	-0.051600	3.252975
264.376459	3514.118237	17.093491	-0.051587	3.249494
264.153256	3506.172903	17.098496	-0.051540	3.246039
264.232716	3498.199771	17.103501	-0.051550	3.242579
264.135090	3490.192531	17.108506	-0.051527	3.239094
264.341231	3482.223347	17.113511	-0.051560	3.235634
263.983902	3474.170629	17.118515	-0.051488	3.232111
264.003653	3466.160681	17.123520	-0.051487	3.228618
264.091764	3458.170927	17.128525	-0.051498	3.225133
263.756661	3450.235491	17.133530	-0.051430	3.221651
263.894328	3442.241281	17.138535	-0.051451	3.218158
263.724051	3434.242373	17.143539	-0.051414	3.214647
263.590220	3426.264540	17.148544	-0.051384	3.211143
263.481436	3418.293849	17.153549	-0.051358	3.207639
263.434582	3410.279258	17.158554	-0.051345	3.204115
263.620059	3402.315492	17.163559	-0.051374	3.200618
263.310510	3394.331890	17.168563	-0.051311	3.197089
263.398555	3386.316186	17.173568	-0.051322	3.193558
263.574077	3378.292549	17.178573	-0.051350	3.190023
263.359920	3370.315369	17.183578	-0.051305	3.186489
263.364520	3362.345410	17.188583	-0.051300	3.182963
263.042377	3354.382277	17.193587	-0.051235	3.179422
263.156562	3346.405557	17.198592	-0.051251	3.175890
263.087705	3338.404544	17.203597	-0.051233	3.172335
263.225931	3330.363216	17.208602	-0.051254	3.168767
263.033448	3322.428540	17.213607	-0.051213	3.165229
262.975070	3314.435298	17.218611	-0.051197	3.161666
262.941912	3306.452167	17.223616	-0.051186	3.158105
262.776816	3298.477520	17.228621	-0.051150	3.154538
262.684106	3290.435162	17.233626	-0.051127	3.150939
262.889167	3282.460341	17.238631	-0.051160	3.147380
262.785284	3274.466638	17.243635	-0.051136	3.143795
262.574345	3266.535665	17.248640	-0.051091	3.140229
262.399155	3258.563066	17.253645	-0.051054	3.136641
262.486181	3250.516439	17.258650	-0.051065	3.133028
262.514039	3242.525754	17.263655	-0.051065	3.129434
262.318363	3234.575174	17.268659	-0.051023	3.125843
262.408600	3226.591888	17.273664	-0.051035	3.122246
262.278192	3218.616691	17.278669	-0.051005	3.118639
261.991271	3210.627588	17.283674	-0.050947	3.115014
262.099940	3202.610190	17.288679	-0.050962	3.111390
261.947023	3194.636262	17.293683	-0.050928	3.107770
262.029189	3186.608478	17.298688	-0.050938	3.104132
261.935237	3178.674219	17.303693	-0.050916	3.100524
261.953091	3170.682525	17.308698	-0.050914	3.096890
261.887310	3162.693479	17.313703	-0.050896	3.093250
261.595417	3154.687897	17.318707	-0.050837	3.089588
261.601321	3146.719534	17.323712	-0.050833	3.085951
261.934273	3138.724979	17.328717	-0.050890	3.082314
261.673555	3130.742149	17.333722	-0.050836	3.078650
261.548153	3122.811175	17.338727	-0.050808	3.075012
261.559272	3114.700302	17.343731	-0.050804	3.071294
261.525846	3106.711139	17.348736	-0.050793	3.067624
261.307085	3098.746959	17.353741	-0.050747	3.063953
261.213954	3090.795264	17.358746	-0.050725	3.060290
261.407244	3082.822625	17.363751	-0.050755	3.056625
261.320284	3074.821753	17.368755	-0.050734	3.052931
261.264386	3066.815955	17.373760	-0.050718	3.049230
261.170929	3058.875031	17.378765	-0.050696	3.045554
261.091005	3050.892488	17.383770	-0.050676	3.041854
261.083407	3042.934477	17.388775	-0.050669	3.038165
261.003989	3034.926979	17.393779	-0.050649	3.034445
261.072741	3026.906671	17.398784	-0.050657	3.030721
261.083090	3018.941119	17.403789	-0.050654	3.027016
261.012491	3010.951503	17.408794	-0.050636	3.023291
260.889409	3002.993943	17.413799	-0.050607	3.019573
260.650264	2995.030251	17.418803	-0.050558	3.015843
260.739721	2987.007615	17.423808	-0.050569	3.012096
260.831291	2979.002693	17.428813	-0.050581	3.008353
260.612248	2971.014199	17.433818	-0.050535	3.004598
260.541947	2963.103996	17.438823	-0.050517	3.000882
260.395975	2955.114626	17.443827	-0.050485	2.997121
260.430018	2947.093230	17.448832	-0.050486	2.993348
260.454616	2939.090871	17.453837	-0.050485	2.989580
260.318556	2931.106283	17.458842	-0.050455	2.985807
260.238056	2923.138538	17.463847	-0.050435	2.982040
260.081281	2915.188983	17.468851	-0.050400	2.978273
260.163444	2907.184681	17.473856	-0.050410	2.974487
260.149321	2899.189573	17.478861	-0.050403	2.970696
259.899816	2891.206741	17.483866	-0.050351	2.966894
259.851888	2883.259376	17.488871	-0.050337	2.963114
259.977506	2875.257084	17.493875	-0.050355	2.959312
260.072745	2867.289215	17.498880	-0.050368	2.955520
259.985836	2859.288940	17.503885	-0.050346	2.951699
259.964734	2851.259349	17.508890	-0.050337	2.947861
259.840835	2843.325643	17.513895	-0.050309	2.944060
259.818371	2835.326176	17.518899	-0.050300	2.940227
259.742755	2827.370217	17.523904	-0.050280	2.936407
259.630384	2819.383803	17.528909	-0.050254	2.932566
259.537613	2811.381783	17.533914	-0.050232	2.928713
259.528039	2803.396857	17.538919	-0.050225	2.924868
259.326316	2795.460172	17.543923	-0.050182	2.921030
259.386708	2787.493170	17.548928	-0.050188	2.917187
259.420521	2779.440151	17.553933	-0.050190	2.913296
259.276849	2771.414714	17.558938	-0.050158	2.909403
259.209339	2763.463192	17.563943	-0.050140	2.905545
259.050776	2755.500768	17.568947	-0.050105	2.901672
258.922774	2747.534144	17.573952	-0.050076	2.897794
258.959634	2739.546629	17.578957	-0.050078	2.893908
258.764162	2731.560254	17.583962	-0.050036	2.890006
258.983146	2723.581780	17.588967	-0.050072	2.886124
258.871560	2715.610954	17.593971	-0.050046	2.882223
258.958230	2707.635994	17.598976	-0.050057	2.878326
258.968916	2699.663680	17.603981	-0.050054	2.874420
258.711179	2691.660231	17.608986	-0.050001	2.870479
258.621609	2683.708845	17.613991	-0.049979	2.866568
258.606000	2675.704293	17.618995	-0.049971	2.862629
258.469678	2667.757208	17.624000	-0.049940	2.858706
258.649943	2659.755885	17.629005	-0.049969	2.854768
258.433472	2651.773438	17.634010	-0.049923	2.850813
258.249657	2643.817432	17.639015	-0.049884	2.846866
258.285833	2635.823202	17.644019	-0.049885	2.842908
258.293200	2627.871010	17.649024	-0.049882	2.838963
258.114985	2619.909407	17.654029	-0.049843	2.834998
257.945392	2611.864625	17.659034	-0.049807	2.830986
258.011368	2603.881629	17.664039	-0.049814	2.827013
258.026802	2595.892427	17.669043	-0.049811	2.823028
258.010763	2587.921204	17.674048	-0.049803	2.819045
257.841569	2579.986834	17.679053	-0.049767	2.815065
257.868758	2571.962876	17.684058	-0.049767	2.811047
257.859749	2564.011104	17.689063	-0.049760	2.807057
257.596176	2556.050779	17.694067	-0.049705	2.803042
257.737578	2548.059831	17.699072	-0.049727	2.799029
257.737413	2540.089121	17.704077	-0.049721	2.795013
257.429309	2532.096732	17.709082	-0.049659	2.790961
257.583111	2524.103541	17.714087	-0.049682	2.786931
257.619780	2516.132905	17.719091	-0.049684	2.782899
257.368555	2508.177598	17.724096	-0.049632	2.778852
257.317898	2500.216280	17.729101	-0.049618	2.774808
257.306430	2492.203736	17.734106	-0.049610	2.770735
257.353126	2484.242785	17.739111	-0.049614	2.766685
257.382901	2476.258108	17.744115	-0.049614	2.762616
257.136636	2468.300309	17.749120	-0.049563	2.758538
257.438842	2460.302449	17.754125	-0.049614	2.754467
257.180195	2452.244286	17.759130	-0.049561	2.750325
257.146302	2444.306457	17.764135	-0.049550	2.746252
257.042686	2436.363716	17.769139	-0.049525	2.742166
256.875738	2428.401513	17.774144	-0.049489	2.738061
256.845866	2420.437598	17.779149	-0.049478	2.733956
256.955590	2412.388139	17.784154	-0.049493	2.729810
256.815525	2404.462518	17.789159	-0.049462	2.725706
256.513577	2396.522890	17.794163	-0.049401	2.721579
256.525238	2388.556430	17.799168	-0.049398	2.717450
256.513859	2380.563340	17.804173	-0.049391	2.713301
256.310781	2372.564515	17.809178	-0.049348	2.709130
256.463791	2364.595546	17.814183	-0.049371	2.704990
256.499241	2356.621631	17.819187	-0.049372	2.700834
256.420577	2348.668252	17.824192	-0.049353	2.696675
256.258813	2340.699577	17.829197	-0.049317	2.692497
256.404278	2332.685624	17.834202	-0.049339	2.688307
256.311242	2324.759140	17.839207	-0.049317	2.684142
256.078696	2316.803648	17.844211	-0.049268	2.679946
256.046131	2308.830685	17.849216	-0.049257	2.675748
256.047828	2300.821732	17.854221	-0.049252	2.671525
255.779779	2292.830330	17.859226	-0.049197	2.667289
255.703233	2284.878101	17.864231	-0.049178	2.663078
255.783102	2276.885335	17.869235	-0.049188	2.658849
255.714515	2268.934467	17.874240	-0.049170	2.654626
255.625334	2260.961815	17.879245	-0.049148	2.650384
255.546494	2252.969066	17.884250	-0.049128	2.646125
255.636034	2245.020139	17.889255	-0.049140	2.641893
255.419083	2237.070300	17.894259	-0.049094	2.637633
255.385917	2229.081726	17.899264	-0.049083	2.633359
255.473889	2221.094173	17.904269	-0.049094	2.629085
255.410471	2213.103875	17.909274	-0.049077	2.624794
255.261608	2205.176964	17.914279	-0.049044	2.620523
255.354642	2197.202785	17.919283	-0.049056	2.616237
255.226096	2189.219542	17.924288	-0.049027	2.611923
255.235413	2181.241733	17.929293	-0.049024	2.607615
255.054424	2173.286569	17.934298	-0.048985	2.603299
255.038645	2165.345771	17.939303	-0.048977	2.598995
254.748469	2157.395945	17.944307	-0.048918	2.594660
254.781950	2149.198384	17.949312	-0.048919	2.590205
254.911879	2141.251993	17.954317	-0.048938	2.585885
254.527881	2133.356434	17.959322	-0.048861	2.581552
254.546962	2125.418200	17.964327	-0.048859	2.577215
254.560107	2117.431947	17.969331	-0.048857	2.572844
254.430498	2109.460678	17.974336	-0.048827	2.568464
254.632068	2101.494941	17.979341	-0.048860	2.564102
254.367468	2093.573278	17.984346	-0.048805	2.559725
254.357865	2085.634288	17.989351	-0.048799	2.555349
254.302206	2077.635339	17.994355	-0.048783	2.550928
254.412018	2069.635553	17.999360	-0.048798	2.546512
254.494049	2061.676177	18.004365	-0.048808	2.542107
254.159231	2053.756462	18.009370	-0.048741	2.537688
254.103409	2045.796486	18.014375	-0.048725	2.533259
254.192853	2037.792485	18.019379	-0.048737	2.528807
254.086218	2029.836739	18.024384	-0.048712	2.524361
253.980005	2021.909806	18.029389	-0.048687	2.519923
254.072740	2013.931344	18.034394	-0.048699	2.515462
254.142221	2005.912394	18.039399	-0.048707	2.510970
253.824132	1997.973556	18.044403	-0.048643	2.506486
253.759043	1990.011350	18.049408	-0.048625	2.501999
253.942076	1982.050068	18.054413	-0.048654	2.497523
253.403905	1974.130715	18.059418	-0.048549	2.493009
253.360440	1966.143179	18.064423	-0.048536	2.488486
253.382037	1958.159856	18.069427	-0.048535	2.483960
253.409649	1950.187261	18.074432	-0.048535	2.479434
253.270176	1942.271962	18.079437	-0.048503	2.474919
253.257732	1934.246371	18.084442	-0.048496	2.470342
253.347558	1926.282971	18.089447	-0.048508	2.465801
253.178781	1918.349592	18.094451	-0.048471	2.461248
253.157679	1910.387522	18.099456	-0.048462	2.456682
253.093041	1902.431285	18.104461	-0.048445	2.452107
252.905491	1894.456951	18.109466	-0.048405	2.447504
252.817019	1886.499089	18.114471	-0.048383	2.442910
252.809017	1878.551630	18.119475	-0.048376	2.438319
252.824755	1870.565626	18.124480	-0.048374	2.433698
252.765366	1862.554357	18.129485	-0.048358	2.429049
252.603919	1854.592307	18.134490	-0.048323	2.424411
252.861533	1846.632624	18.139495	-0.048366	2.419798
252.631346	1838.721922	18.144499	-0.048318	2.415167
252.410880	1830.758251	18.149504	-0.048271	2.410497
252.527784	1822.790473	18.154509	-0.048288	2.405841
252.443671	1814.852219	18.159514	-0.048267	2.401179
252.314393	1806.920838	18.164519	-0.048238	2.396507
252.171310	1798.936652	18.169523	-0.048206	2.391795
252.186941	1790.958757	18.174528	-0.048204	2.387089
252.203336	1782.994626	18.179533	-0.048202	2.382382
251.981867	1775.063274	18.184538	-0.048156	2.377666
252.066244	1767.092390	18.189543	-0.048166	2.372942
251.992958	1759.136953	18.194547	-0.048147	2.368205
251.876199	1751.191795	18.199552	-0.048120	2.363461
251.944573	1743.249512	18.204557	-0.048128	2.358724
251.763438	1735.284011	18.209562	-0.048089	2.353944
251.710532	1727.299040	18.214567	-0.048074	2.349153
251.611543	1719.351924	18.219571	-0.048051	2.344370
251.565702	1711.391872	18.224576	-0.048037	2.339575
251.659845	1703.452724	18.229581	-0.048049	2.334793
251.680861	1695.455841	18.234586	-0.048048	2.329961
251.438035	1687.540710	18.239591	-0.047998	2.325147
251.467380	1679.596622	18.244595	-0.047998	2.320328
251.214985	1671.668675	18.249600	-0.047946	2.315485
251.279480	1663.689684	18.254605	-0.047953	2.310627
251.172205	1655.714376	18.259610	-0.047928	2.305746
251.215039	1647.786430	18.264615	-0.047930	2.300897
251.255981	1639.829909	18.269619	-0.047933	2.296020
251.073280	1631.877558	18.274624	-0.047894	2.291116
251.181131	1623.906477	18.279629	-0.047909	2.286215
250.989820	1615.981438	18.284634	-0.047868	2.281306
250.909836	1608.045886	18.289639	-0.047848	2.276390
250.934996	1600.032788	18.294643	-0.047848	2.271424
250.739573	1592.069667	18.299648	-0.047806	2.266459
250.742868	1584.135934	18.304653	-0.047801	2.261519
250.645800	1576.193702	18.309658	-0.047778	2.256553
250.577967	1568.251985	18.314663	-0.047760	2.251580
250.663483	1560.277690	18.319667	-0.047771	2.246589
250.289552	1552.380002	18.324672	-0.047697	2.241594
250.480480	1544.438304	18.329677	-0.047727	2.236610
250.247349	1536.477953	18.334682	-0.047678	2.231566
250.288599	1528.500868	18.339687	-0.047681	2.226524
250.186551	1520.589156	18.344691	-0.047657	2.221499
249.932582	1512.669325	18.349696	-0.047604	2.216444
249.998358	1504.698384	18.354701	-0.047612	2.211374
249.830856	1496.752298	18.359706	-0.047575	2.206287
249.937744	1488.794572	18.364711	-0.047590	2.201205
249.881338	1480.866705	18.369715	-0.047574	2.196116
249.831293	1472.902976	18.374720	-0.047560	2.190993
249.756618	1464.955081	18.379725	-0.047541	2.185865
249.482924	1457.041711	18.384730	-0.047485	2.180730
249.576091	1449.081949	18.389735	-0.047497	2.175586
249.619052	1441.125222	18.394739	-0.047500	2.170427
249.382771	1433.196342	18.399744	-0.047451	2.165248
249.638518	1425.253673	18.404749	-0.047493	2.160094
249.399837	1417.336954	18.409754	-0.047444	2.154898
249.419569	1409.377405	18.414759	-0.047442	2.149685
249.153427	1401.462285	18.419763	-0.047387	2.144462
249.028469	1393.524410	18.424768	-0.047359	2.139225
249.124349	1385.575369	18.429773	-0.047372	2.133988
248.937460	1377.629500	18.434778	-0.047332	2.128714
248.798145	1369.714009	18.439783	-0.047301	2.123451
248.911475	1361.779321	18.444787	-0.047317	2.118187
248.846178	1353.802021	18.449792	-0.047299	2.112864
248.836755	1345.826532	18.454797	-0.047293	2.107534
248.543997	1337.918391	18.459802	-0.047233	2.102208
248.605756	1329.987369	18.464807	-0.047239	2.096887
248.449243	1322.052893	18.469811	-0.047205	2.091530
248.472275	1314.101275	18.474816	-0.047204	2.086165
248.526958	1306.193354	18.479821	-0.047209	2.080818
248.422415	1298.268635	18.484826	-0.047185	2.075431
248.364569	1290.317880	18.489831	-0.047169	2.070016
248.425571	1282.371319	18.494835	-0.047175	2.064602
248.341736	1274.473047	18.499840	-0.047154	2.059193
248.275375	1266.552548	18.504845	-0.047137	2.053755
248.147854	1258.605992	18.509850	-0.047108	2.048279
248.152373	1250.681548	18.514855	-0.047104	2.042817
247.844174	1242.813763	18.519859	-0.047041	2.037348
247.675402	1234.871268	18.524864	-0.047005	2.031826
247.803900	1226.891948	18.529869	-0.047023	2.026294
247.691052	1218.974754	18.534874	-0.046997	2.020765
247.696682	1211.047320	18.539879	-0.046993	2.015227
247.682205	1203.108578	18.544883	-0.046985	2.009663
247.532270	1195.195859	18.549888	-0.046952	2.004087
247.471715	1187.300650	18.554893	-0.046936	1.998518
247.370606	1179.360235	18.559898	-0.046912	1.992897
247.520494	1171.400185	18.564903	-0.046935	1.987273
247.311038	1163.517020	18.569907	-0.046891	1.981649
247.263457	1155.597507	18.574912	-0.046877	1.976001
247.565937	1147.626244	18.579917	-0.046928	1.970336
247.265857	1139.736638	18.584922	-0.046867	1.964650
247.100046	1131.861311	18.589927	-0.046831	1.958971
246.997132	1123.935299	18.594931	-0.046807	1.953246
246.983839	1115.957714	18.599936	-0.046799	1.947477
247.002062	1108.047386	18.604941	-0.046797	1.941743
246.859691	1100.136916	18.609946	-0.046766	1.935974
246.818520	1092.219939	18.614951	-0.046753	1.930194
246.665025	1084.321432	18.619955	-0.046719	1.924398
246.391054	1076.450111	18.624960	-0.046663	1.918591
246.408471	1068.530679	18.629965	-0.046661	1.912764
246.373467	1060.573387	18.634970	-0.046650	1.906884
246.284722	1052.685800	18.639975	-0.046628	1.901032
246.334135	1044.764268	18.644979	-0.046632	1.895153
246.215757	1036.847732	18.649984	-0.046605	1.889240
246.138631	1028.956454	18.654989	-0.046585	1.883331
246.259635	1021.029911	18.659994	-0.046603	1.877401
246.016833	1013.145348	18.664999	-0.046553	1.871441
246.162446	1005.194023	18.670003	-0.046575	1.865457
246.011444	997.316827	18.675008	-0.046541	1.859475
245.988388	989.426436	18.680013	-0.046532	1.853479
245.854448	981.517386	18.685018	-0.046502	1.847436
245.639398	973.645498	18.690023	-0.046457	1.841392
245.584562	965.763039	18.695027	-0.046441	1.835339
245.615878	957.809935	18.700032	-0.046442	1.829221
245.502499	949.939525	18.705037	-0.046416	1.823130
245.630860	942.006761	18.710042	-0.046435	1.816999
245.624572	934.101332	18.715047	-0.046428	1.810852
245.455352	926.234479	18.720051	-0.046392	1.804695
245.248712	918.377474	18.725056	-0.046348	1.798520
245.136203	910.468156	18.730061	-0.046322	1.792294
245.322319	902.486527	18.735066	-0.046352	1.786025
245.095114	894.644507	18.740071	-0.046304	1.779794
245.121920	886.752174	18.745075	-0.046304	1.773533
245.000425	878.850263	18.750080	-0.046277	1.767223
244.922878	870.997082	18.755085	-0.046257	1.760936
244.698938	863.135178	18.760090	-0.046210	1.754600
244.660419	855.231667	18.765095	-0.046198	1.748231
244.615962	847.348039	18.770099	-0.046185	1.741854
244.309102	839.509369	18.775104	-0.046122	1.735457
244.472767	831.587263	18.780109	-0.046148	1.729028
244.549943	823.683003	18.785114	-0.046157	1.722579
244.169790	815.871317	18.790119	-0.046081	1.716123
244.085685	807.975418	18.795123	-0.046060	1.709611
243.933620	800.095073	18.800128	-0.046027	1.703078
244.188677	792.192139	18.805133	-0.046069	1.696554
244.104949	784.308423	18.810138	-0.046049	1.689977
244.089818	776.436571	18.815143	-0.046041	1.683393
244.073673	768.577816	18.820147	-0.046033	1.676794
243.760989	760.733895	18.825152	-0.045969	1.670142
243.927464	752.840140	18.830157	-0.045995	1.663485
243.881580	744.982318	18.835162	-0.045982	1.656803
243.785072	737.119481	18.840167	-0.045959	1.650084
243.638182	729.287636	18.845171	-0.045926	1.643356
243.591098	721.428385	18.850176	-0.045912	1.636591
243.565453	713.521709	18.855181	-0.045903	1.629759
243.248415	705.679250	18.860186	-0.045838	1.622914
243.299330	697.822555	18.865191	-0.045843	1.616079
243.351441	689.946240	18.870195	-0.045847	1.609198
243.203040	682.111697	18.875200	-0.045815	1.602296
243.164302	674.285625	18.880205	-0.045803	1.595387
242.837185	666.456088	18.885210	-0.045737	1.588404
243.044444	658.564072	18.890215	-0.045770	1.581411
242.916956	650.757805	18.895219	-0.045741	1.574415
242.799403	642.897263	18.900224	-0.045714	1.567340
242.658737	635.098271	18.905229	-0.045683	1.560286
242.392519	627.287194	18.910234	-0.045628	1.553170
242.361223	619.415756	18.915239	-0.045618	1.546001
242.430116	611.572207	18.920243	-0.045625	1.538839
242.175683	603.762377	18.925248	-0.045573	1.531626
242.290593	595.907948	18.930253	-0.045589	1.524394
242.183752	588.100613	18.935258	-0.045564	1.517137
242.057152	580.280077	18.940263	-0.045536	1.509830
241.980445	572.463715	18.945267	-0.045516	1.502498
241.931254	564.637654	18.950272	-0.045502	1.495126
241.823935	556.832155	18.955277	-0.045477	1.487728
241.612252	549.046216	18.960282	-0.045433	1.480295
241.475619	541.232965	18.965287	-0.045402	1.472810
241.493935	533.371168	18.970291	-0.045400	1.465265
241.407930	525.576384	18.975296	-0.045379	1.457729
241.479944	517.754530	18.980301	-0.045388	1.450152
241.273238	509.976592	18.985306	-0.045344	1.442534
241.199045	502.205355	18.990311	-0.045325	1.434903
241.161460	494.394214	18.995315	-0.045313	1.427198
240.851490	486.650681	19.000320	-0.045251	1.419474
241.026171	478.822437	19.005325	-0.045278	1.411703
240.807255	471.059673	19.010330	-0.045232	1.403889
240.759642	463.291668	19.015335	-0.045218	1.396055
240.516288	455.527622	19.020339	-0.045168	1.388147
240.367707	447.752098	19.025344	-0.045135	1.380198
240.356249	439.983754	19.030349	-0.045128	1.372234
240.181236	432.222540	19.035354	-0.045091	1.364203
240.234992	424.452202	19.040359	-0.045096	1.356155
240.235202	416.673607	19.045363	-0.045091	1.348040
239.902515	408.960896	19.050368	-0.045024	1.339887
239.974459	401.196477	19.055373	-0.045032	1.331701
239.689229	393.480529	19.060378	-0.044974	1.323452
239.767034	385.710696	19.065383	-0.044984	1.315158
239.783725	377.833984	19.070387	-0.044982	1.306686
239.614838	370.133939	19.075392	-0.044945	1.298317
239.569009	362.417829	19.080397	-0.044932	1.289898
239.430010	354.711307	19.085402	-0.044901	1.281417
239.311614	347.016797	19.090407	-0.044874	1.272896
239.303856	339.291620	19.095411	-0.044867	1.264305
239.194494	331.598561	19.100416	-0.044842	1.255672
239.098560	323.908510	19.105421	-0.044819	1.246985
238.616074	316.292282	19.110426	-0.044724	1.238247
238.485231	308.583718	19.115431	-0.044695	1.229408
238.372697	300.898581	19.120435	-0.044669	1.220536
238.416994	293.188490	19.125440	-0.044672	1.211601
238.229702	285.544947	19.130445	-0.044633	1.202632
238.159361	277.878313	19.135450	-0.044615	1.193592
238.146934	270.199688	19.140455	-0.044607	1.184479
237.994934	262.569995	19.145459	-0.044574	1.175327
237.740661	254.938954	19.150464	-0.044522	1.166079
237.669760	247.320266	19.155469	-0.044504	1.156811
237.162679	239.709731	19.160474	-0.044404	1.147386
236.804335	232.119504	19.165479	-0.044333	1.137940
236.850545	224.469223	19.170483	-0.044336	1.128426
236.437935	216.911359	19.175488	-0.044255	1.118849
235.908484	209.375062	19.180493	-0.044151	1.109190
235.645713	201.791510	19.185498	-0.044097	1.099444
235.385816	194.217862	19.190503	-0.044044	1.089625
235.058235	186.678278	19.195507	-0.043978	1.079746
234.300917	179.192287	19.200512	-0.043832	1.069748
234.132907	171.623663	19.205517	-0.043796	1.059680
233.627237	164.126596	19.210522	-0.043697	1.049534
233.033828	156.644922	19.215527	-0.043582	1.039289
232.876033	149.099228	19.220531	-0.043548	1.028957
232.354514	141.624314	19.225536	-0.043446	1.018531
231.876441	134.161940	19.230541	-0.043352	1.008025
231.363247	126.711309	19.235546	-0.043251	0.997416
231.082721	119.193267	19.240551	-0.043194	0.986654
230.677975	111.753807	19.245555	-0.043114	0.975856
230.167576	104.327981	19.250560	-0.043014	0.964929
229.796869	96.923836	19.255565	-0.042941	0.953945
229.316401	89.524438	19.260570	-0.042846	0.942812
228.785121	82.166412	19.265575	-0.042743	0.931594
228.386841	74.803199	19.270579	-0.042664	0.920267
227.695153	67.492529	19.275584	-0.042530	0.908801
227.250310	60.397521	19.280589	-0.042443	0.897594