Tue Mar 23 11:01:06 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.860477	-0.062537	0.000000	-0.000069	0.722376

0.631031	-0.023438	0.005005	-0.000027	0.722373
0.701628	-0.034097	0.010010	-0.000040	0.722377
0.633422	-0.026723	0.015014	-0.000027	0.722368
0.634786	-0.023905	0.020019	-0.000028	0.722374
0.552816	-0.009947	0.025024	-0.000012	0.722373
0.569543	-0.013877	0.030029	-0.000016	0.722371
0.756201	-0.043887	0.035034	-0.000050	0.722377
0.554284	-0.011636	0.040038	-0.000013	0.722370
0.618578	-0.018709	0.045043	-0.000025	0.722379
0.687122	-0.034010	0.050048	-0.000038	0.722373
0.991817	-0.091351	0.055053	-0.000095	0.722367
0.909309	-0.074198	0.060058	-0.000079	0.722372
0.614663	-0.024167	0.065062	-0.000025	0.722368
0.822211	-0.175898	0.070067	-0.000063	0.722142
0.472573	-0.146900	0.075072	0.000002	0.722077
0.340319	-0.124705	0.080077	0.000026	0.722075
0.586486	-0.165708	0.085082	-0.000020	0.722080
0.498568	-0.155100	0.090086	-0.000003	0.722071
0.598784	-0.170001	0.095091	-0.000022	0.722077
0.522878	-0.156526	0.100096	-0.000008	0.722077
0.529604	-0.318717	0.105101	-0.000009	0.721760
0.616601	-0.339524	0.110106	-0.000025	0.721750
0.600192	-0.340453	0.115110	-0.000022	0.721743
0.589379	-0.334557	0.120115	-0.000021	0.721751
0.620247	-0.342433	0.125120	-0.000026	0.721746
0.687122	-0.496527	0.130125	-0.000039	0.721467
0.703006	-0.510704	0.135130	-0.000042	0.721444
0.790992	-0.530575	0.140134	-0.000058	0.721436
0.789186	-0.524934	0.145139	-0.000058	0.721447
0.410132	-0.590850	0.150144	0.000013	0.721185
0.292668	-0.599927	0.155149	0.000034	0.721126
0.275772	-0.593427	0.160154	0.000037	0.721133
0.266322	-0.596186	0.165158	0.000039	0.721124
0.422810	-0.724553	0.170163	0.000010	0.720927
0.255765	-0.718248	0.175168	0.000041	0.720881
0.206276	-0.710269	0.180173	0.000050	0.720879
0.301881	-0.767061	0.185178	0.000032	0.720801
0.193054	-0.879340	0.190182	0.000052	0.720542
0.395543	-0.912102	0.195187	0.000015	0.720549
0.356658	-0.911718	0.200192	0.000022	0.720536
0.467414	-1.089749	0.205197	0.000001	0.720224
0.431716	-1.079351	0.210202	0.000008	0.720232
0.297796	-1.074087	0.215206	0.000033	0.720196
0.360884	-1.232468	0.220211	0.000021	0.719906
0.126811	-1.194354	0.225216	0.000064	0.719899
0.026471	-1.212602	0.230221	0.000083	0.719828
0.047470	-1.327788	0.235226	0.000079	0.719609
0.237742	-1.365704	0.240230	0.000044	0.719601
0.274304	-1.455767	0.245235	0.000037	0.719436
0.319647	-1.548127	0.250240	0.000028	0.719270
0.369617	-1.563631	0.255245	0.000019	0.719257
0.201580	-1.680825	0.260250	0.000050	0.718967
0.207950	-1.686942	0.265254	0.000049	0.718958
0.340302	-1.809526	0.270259	0.000024	0.718762
0.347805	-1.871904	0.275264	0.000023	0.718642
0.052958	-1.874108	0.280269	0.000078	0.718534
0.009612	-1.953809	0.285274	0.000086	0.718362
0.191705	-2.007375	0.290278	0.000052	0.718320
0.166754	-2.154792	0.295283	0.000056	0.718020
-0.032703	-2.118956	0.300288	0.000094	0.718021
-0.053740	-2.266414	0.305293	0.000097	0.717722
0.215496	-2.320044	0.310298	0.000047	0.717711
-0.249860	-2.381839	0.315302	0.000134	0.717425
-0.336689	-2.386857	0.320307	0.000150	0.717385
-1.590767	-2.272302	0.325312	0.000383	0.717170
-3.219271	-2.024925	0.330317	0.000686	0.717086
-2.626570	-2.127520	0.335322	0.000576	0.717092
-3.051314	-2.187774	0.340326	0.000655	0.716823
-4.137876	-2.024032	0.345331	0.000857	0.716764
-3.735075	-2.098883	0.350336	0.000782	0.716758
-3.948348	-2.130635	0.355341	0.000822	0.716620
-5.191270	-1.994364	0.360346	0.001053	0.716452
-4.774315	-2.071065	0.365350	0.000975	0.716447
-4.525445	-2.112433	0.370355	0.000929	0.716453
-5.086299	-2.105533	0.375360	0.001033	0.716269
-5.960045	-2.019288	0.380365	0.001196	0.716132
-5.418417	-2.110947	0.385370	0.001095	0.716141
-6.089493	-1.998320	0.390374	0.001220	0.716128
-5.720722	-2.087788	0.395379	0.001151	0.716081
-5.988371	-2.139631	0.400384	0.001201	0.715884
-6.185171	-2.105210	0.405389	0.001237	0.715883
-6.643496	-2.019328	0.410394	0.001323	0.715891
-6.421672	-2.063639	0.415398	0.001281	0.715882
-6.663007	-2.156115	0.420403	0.001326	0.715614
-7.684841	-2.007728	0.425408	0.001516	0.715547
-7.778437	-1.992514	0.430413	0.001534	0.715544
-7.176554	-2.096565	0.435418	0.001421	0.715551
-7.665434	-2.014057	0.440422	0.001512	0.715542
-7.674594	-2.114534	0.445427	0.001514	0.715339
-8.445502	-2.032065	0.450432	0.001657	0.715231
-8.544661	-2.017393	0.455437	0.001676	0.715225
-8.466681	-2.025578	0.460442	0.001661	0.715237
-8.512249	-2.022497	0.465446	0.001670	0.715227
-8.154047	-2.084330	0.470451	0.001603	0.715231
-8.790749	-2.127958	0.475456	0.001721	0.714919
-9.340065	-2.036053	0.480461	0.001824	0.714908
-8.931345	-2.104685	0.485466	0.001747	0.714916
-8.948623	-2.107976	0.490470	0.001751	0.714904
-9.592920	-1.990346	0.495475	0.001870	0.714909
-9.293381	-2.061077	0.500480	0.001815	0.714875
-9.827525	-2.103041	0.505485	0.001914	0.714603
-10.158488	-2.040160	0.510490	0.001975	0.714611
-10.652427	-1.955756	0.515494	0.002067	0.714604
-10.177507	-2.036969	0.520499	0.001979	0.714611
-10.043729	-2.061465	0.525504	0.001954	0.714610
-10.418102	-1.998712	0.530509	0.002023	0.714602
-10.147010	-2.148574	0.535514	0.001973	0.714400
-11.539385	-1.964043	0.540518	0.002232	0.714274
-11.289473	-2.007419	0.545523	0.002185	0.714277
-10.805540	-2.094327	0.550528	0.002095	0.714276
-11.249758	-2.018343	0.555533	0.002178	0.714270
-10.987104	-2.059000	0.560538	0.002129	0.714282
-10.975653	-2.068582	0.565542	0.002127	0.714267
-11.547895	-2.114628	0.570547	0.002233	0.713973
-11.799113	-2.069722	0.575552	0.002280	0.713974
-12.600772	-1.929868	0.580557	0.002429	0.713968
-11.702326	-2.085745	0.585562	0.002262	0.713976
-11.826772	-2.069310	0.590566	0.002285	0.713965
-12.216974	-1.996624	0.595571	0.002357	0.713972
-12.240952	-2.023290	0.600576	0.002362	0.713910
-13.045542	-2.011895	0.605581	0.002511	0.713648
-12.728677	-2.064571	0.610586	0.002452	0.713656
-13.351119	-1.957893	0.615590	0.002568	0.713647
-13.129917	-1.991959	0.620595	0.002527	0.713658
-12.853567	-2.044090	0.625600	0.002475	0.713653
-13.137492	-1.995829	0.630605	0.002528	0.713648
-12.605108	-2.088309	0.635610	0.002429	0.713653
-13.495877	-2.078575	0.640614	0.002595	0.713357
-13.969363	-1.990269	0.645619	0.002683	0.713365
-13.744532	-2.031064	0.650624	0.002641	0.713364
-13.712590	-2.039893	0.655629	0.002635	0.713358
-14.114003	-1.965052	0.660634	0.002709	0.713364
-14.246085	-1.944897	0.665638	0.002734	0.713358
-13.853920	-2.012638	0.670643	0.002661	0.713362
-14.223581	-2.075118	0.675648	0.002730	0.713107
-15.265060	-1.932329	0.680653	0.002923	0.713022
-14.664225	-2.035716	0.685658	0.002812	0.713029
-14.464981	-2.075287	0.690662	0.002774	0.713021
-14.999348	-1.977664	0.695667	0.002874	0.713026
-14.935880	-1.991087	0.700672	0.002862	0.713022
-14.982490	-1.985058	0.705677	0.002870	0.713018
-14.670256	-2.112581	0.710682	0.002812	0.712875
-15.962821	-1.967686	0.715686	0.003053	0.712705
-15.558196	-2.036946	0.720691	0.002977	0.712711
-15.452362	-2.055212	0.725696	0.002958	0.712712
-15.898433	-1.980137	0.730701	0.003041	0.712704
-15.469098	-2.051918	0.735706	0.002961	0.712713
-15.654333	-2.023504	0.740710	0.002995	0.712704
-15.819765	-2.079379	0.745715	0.003026	0.712534
-16.567925	-2.019787	0.750720	0.003165	0.712388
-16.200800	-2.086130	0.755725	0.003097	0.712386
-16.677543	-1.996186	0.760730	0.003185	0.712396
-16.965385	-1.950783	0.765734	0.003239	0.712385
-16.508275	-2.027398	0.770739	0.003153	0.712394
-16.368501	-2.054923	0.775744	0.003127	0.712389
-17.152740	-1.969853	0.780749	0.003273	0.712281
-17.757712	-1.955552	0.785754	0.003386	0.712094
-17.137986	-2.070460	0.790758	0.003270	0.712086
-17.522605	-1.998572	0.795763	0.003342	0.712093
-17.532760	-1.996254	0.800768	0.003344	0.712094
-17.376985	-2.027687	0.805773	0.003315	0.712086
-17.427167	-2.015458	0.810778	0.003324	0.712093
-17.748455	-1.961313	0.815782	0.003384	0.712087
-18.180851	-2.046302	0.820787	0.003464	0.711764
-18.302335	-2.023759	0.825792	0.003487	0.711766
-18.857235	-1.929010	0.830797	0.003590	0.711758
-18.237901	-2.034065	0.835802	0.003474	0.711769
-18.513075	-1.991459	0.840806	0.003526	0.711756
-18.899284	-1.920189	0.845811	0.003597	0.711761
-18.377603	-2.012464	0.850816	0.003500	0.711763
-18.335705	-2.101987	0.855821	0.003492	0.711599
-19.313210	-1.997826	0.860826	0.003674	0.711460
-19.291769	-2.006223	0.865830	0.003670	0.711451
-19.543335	-1.958158	0.870835	0.003717	0.711457
-19.021215	-2.052157	0.875840	0.003620	0.711456
-19.236226	-2.016824	0.880845	0.003660	0.711450
-19.456058	-1.972808	0.885850	0.003700	0.711460
-19.454358	-2.056775	0.890854	0.003700	0.711293
-20.380335	-1.969266	0.895859	0.003872	0.711138
-20.053482	-2.027656	0.900864	0.003811	0.711138
-20.599569	-1.932123	0.905869	0.003913	0.711135
-20.157311	-2.006851	0.910874	0.003831	0.711143
-20.316812	-1.984143	0.915878	0.003860	0.711132
-20.552605	-1.938654	0.920883	0.003904	0.711139
-20.178358	-2.023512	0.925888	0.003834	0.711103
-20.987557	-1.998334	0.930893	0.003985	0.710866
-20.871040	-2.013817	0.935898	0.003963	0.710876
-21.051830	-1.984851	0.940902	0.003997	0.710870
-20.812320	-2.026156	0.945907	0.003952	0.710873
-21.071516	-1.981031	0.950912	0.004000	0.710871
-21.183640	-1.964103	0.955917	0.004021	0.710865
-20.464273	-2.158474	0.960922	0.003887	0.710733
-22.202397	-1.948814	0.965926	0.004210	0.710533
-21.993347	-1.982936	0.970931	0.004172	0.710540
-21.694305	-2.039967	0.975936	0.004116	0.710532
-22.292378	-1.935400	0.980941	0.004227	0.710528
-22.155214	-1.954488	0.985946	0.004201	0.710539
-22.116290	-1.965408	0.990950	0.004194	0.710532
-22.118631	-1.984640	0.995955	0.004194	0.710492
-22.781117	-2.003411	1.000960	0.004318	0.710219
-23.183557	-1.934518	1.005965	0.004393	0.710214
-22.950569	-1.972243	1.010970	0.004349	0.710221
-22.951546	-1.976287	1.015974	0.004349	0.710213
-23.098339	-1.947750	1.020979	0.004376	0.710218
-22.920029	-1.979248	1.025984	0.004343	0.710219
-23.050095	-1.957909	1.030989	0.004367	0.710215
-22.910805	-2.080174	1.035994	0.004341	0.710021
-24.134116	-1.927467	1.040998	0.004569	0.709890
-23.887720	-1.967624	1.046003	0.004523	0.709898
-23.785286	-1.988100	1.051008	0.004504	0.709894
-24.398039	-1.880950	1.056013	0.004618	0.709890
-23.692407	-2.003206	1.061018	0.004486	0.709897
-23.934570	-1.964664	1.066022	0.004531	0.709888
-24.027563	-1.977754	1.071027	0.004549	0.709829
-24.435848	-2.019405	1.076032	0.004625	0.709600
-24.483063	-2.015479	1.081037	0.004633	0.709591
-24.979281	-1.922849	1.086042	0.004726	0.709600
-24.987095	-1.925280	1.091046	0.004727	0.709592
-24.548608	-2.002124	1.096051	0.004645	0.709595
-24.877969	-1.941214	1.101056	0.004706	0.709600
-25.124221	-1.900458	1.106061	0.004752	0.709593
-25.108443	-2.061147	1.111066	0.004749	0.709278
-25.624030	-1.978011	1.116070	0.004845	0.709260
-25.852149	-1.935531	1.121075	0.004888	0.709264
-25.615846	-1.979275	1.126080	0.004843	0.709261
-25.788730	-1.949484	1.131085	0.004876	0.709259
-25.621263	-1.974607	1.136090	0.004844	0.709269
-25.674945	-1.969955	1.141094	0.004854	0.709259
-26.282350	-1.993059	1.146099	0.004967	0.708996
-26.904617	-1.901625	1.151104	0.005083	0.708957
-26.863374	-1.911547	1.156109	0.005075	0.708952
-26.367437	-1.996996	1.161114	0.004983	0.708958
-26.727446	-1.937251	1.166118	0.005050	0.708950
-26.909182	-1.902061	1.171123	0.005084	0.708956
-26.540990	-1.967242	1.176128	0.005015	0.708957
-26.659227	-1.992783	1.181133	0.005037	0.708863
-27.575960	-1.939807	1.186138	0.005207	0.708642
-27.528760	-1.951685	1.191142	0.005199	0.708636
-27.554470	-1.946715	1.196147	0.005203	0.708637
-27.416938	-1.969938	1.201152	0.005178	0.708639
-27.655343	-1.931078	1.206157	0.005222	0.708632
-27.562224	-1.942959	1.211162	0.005204	0.708642
-27.335912	-1.998129	1.216166	0.005162	0.708612
-28.147298	-1.986116	1.221171	0.005313	0.708347
-28.266823	-1.962053	1.226176	0.005335	0.708352
-28.571402	-1.910854	1.231181	0.005392	0.708346
-28.120803	-1.988465	1.236186	0.005308	0.708352
-28.397493	-1.943287	1.241190	0.005360	0.708344
-28.327820	-1.954574	1.246195	0.005346	0.708346
-27.875533	-2.078352	1.251200	0.005262	0.708260
-29.492054	-1.918315	1.256205	0.005563	0.708003
-28.989698	-2.000248	1.261210	0.005469	0.708019
-29.310707	-1.949115	1.266214	0.005529	0.708007
-29.515755	-1.911019	1.271219	0.005567	0.708010
-29.163544	-1.973590	1.276224	0.005502	0.708010
-29.069222	-1.993396	1.281229	0.005484	0.708005
-29.056717	-2.034542	1.286234	0.005482	0.707927
-30.318202	-1.925023	1.291238	0.005716	0.707696
-30.145248	-1.954328	1.296243	0.005684	0.707699
-29.976335	-1.984392	1.301248	0.005653	0.707699
-30.397258	-1.911793	1.306253	0.005731	0.707694
-30.001553	-1.979432	1.311258	0.005657	0.707700
-29.820050	-2.014696	1.316262	0.005623	0.707695
-30.020181	-2.019448	1.321267	0.005660	0.707614
-31.057224	-1.953951	1.326272	0.005853	0.707374
-31.009037	-1.964288	1.331277	0.005844	0.707371
-31.054970	-1.951554	1.336282	0.005853	0.707380
-31.131818	-1.942409	1.341286	0.005867	0.707371
-30.938140	-1.974904	1.346291	0.005831	0.707376
-30.648051	-2.026174	1.351296	0.005777	0.707377
-30.957103	-2.001386	1.356301	0.005834	0.707316
-31.575877	-2.008004	1.361306	0.005949	0.707081
-31.558821	-2.012404	1.366310	0.005946	0.707079
-32.118071	-1.912661	1.371315	0.006050	0.707079
-31.801407	-1.967075	1.376320	0.005991	0.707083
-31.789665	-1.972899	1.381325	0.005989	0.707076
-31.720803	-1.981635	1.386330	0.005976	0.707083
-31.878156	-2.008740	1.391334	0.006005	0.706973
-32.754123	-1.962466	1.396339	0.006168	0.706752
-32.173888	-2.065410	1.401344	0.006060	0.706753
-32.921709	-1.934893	1.406349	0.006199	0.706748
-32.830025	-1.946805	1.411354	0.006182	0.706757
-32.577625	-1.997304	1.416358	0.006135	0.706746
-32.769115	-1.960575	1.421363	0.006171	0.706751
-32.707611	-2.041688	1.426368	0.006159	0.706611
-33.996273	-1.895513	1.431373	0.006399	0.706443
-33.275683	-2.022775	1.436378	0.006265	0.706445
-33.525060	-1.981748	1.441382	0.006311	0.706439
-33.674458	-1.955667	1.446387	0.006339	0.706438
-33.288420	-2.021362	1.451392	0.006267	0.706444
-33.730234	-1.947242	1.456397	0.006349	0.706435
-33.615586	-2.034261	1.461402	0.006328	0.706301
-34.399893	-1.984802	1.466406	0.006473	0.706120
-34.552832	-1.955449	1.471411	0.006502	0.706124
-34.677374	-1.931352	1.476416	0.006525	0.706128
-34.684294	-1.935631	1.481421	0.006526	0.706117
-34.140621	-2.027367	1.486426	0.006425	0.706128
-34.795688	-1.914654	1.491430	0.006547	0.706120
-34.794304	-1.939001	1.496435	0.006546	0.706072
-34.921376	-2.019024	1.501440	0.006570	0.705865
-35.160640	-1.979794	1.506445	0.006614	0.705858
-35.345001	-1.942980	1.511450	0.006649	0.705867
-35.171022	-1.979808	1.516454	0.006616	0.705855
-35.098293	-1.990444	1.521459	0.006603	0.705860
-34.989468	-2.008793	1.526464	0.006582	0.705862
-35.497431	-2.038388	1.531469	0.006677	0.705621
-36.045379	-1.986447	1.536474	0.006779	0.705529
-36.314199	-1.940474	1.541478	0.006829	0.705525
-36.128444	-1.974475	1.546483	0.006794	0.705523
-36.059776	-1.985862	1.551488	0.006781	0.705525
-36.235923	-1.957569	1.556493	0.006814	0.705519
-36.094377	-1.978727	1.561498	0.006787	0.705527
-36.537939	-2.029546	1.566502	0.006870	0.705266
-37.172357	-1.945190	1.571507	0.006988	0.705208
-37.117605	-1.952470	1.576512	0.006978	0.705214
-37.123020	-1.956001	1.581517	0.006979	0.705205
-37.053646	-1.965383	1.586522	0.006966	0.705211
-37.238838	-1.934159	1.591526	0.007000	0.705207
-37.375380	-1.909745	1.596531	0.007025	0.705208
-36.827421	-2.092903	1.601536	0.006923	0.705036
-38.094105	-1.944500	1.606541	0.007159	0.704880
-37.878407	-1.977873	1.611546	0.007119	0.704890
-37.871319	-1.981772	1.616550	0.007117	0.704885
-37.886638	-1.980592	1.621555	0.007120	0.704882
-37.718028	-2.008361	1.626560	0.007089	0.704887
-38.138900	-1.937141	1.631565	0.007167	0.704880
-37.934580	-2.077908	1.636570	0.007129	0.704669
-38.813894	-1.961526	1.641574	0.007292	0.704588
-39.003090	-1.926991	1.646579	0.007328	0.704590
-38.784869	-1.962675	1.651584	0.007287	0.704597
-38.985280	-1.931368	1.656589	0.007324	0.704588
-38.826935	-1.956070	1.661594	0.007295	0.704595
-38.771400	-1.969068	1.666598	0.007284	0.704589
-39.164906	-2.017938	1.671603	0.007357	0.704349
-39.825293	-1.942880	1.676608	0.007480	0.704264
-39.812394	-1.949128	1.681613	0.007478	0.704256
-39.628956	-1.977879	1.686618	0.007444	0.704264
-39.856045	-1.940498	1.691622	0.007486	0.704258
-39.830896	-1.943395	1.696627	0.007481	0.704261
-39.430687	-2.013186	1.701632	0.007406	0.704264
-39.913124	-2.023628	1.706637	0.007496	0.704070
-40.915912	-1.901403	1.711642	0.007683	0.703956
-40.719391	-1.940536	1.716646	0.007646	0.703948
-40.604705	-1.959588	1.721651	0.007625	0.703951
-40.576549	-1.960933	1.726656	0.007619	0.703959
-40.769801	-1.932250	1.731661	0.007655	0.703947
-40.719927	-1.936228	1.736666	0.007646	0.703957
-40.657932	-1.988285	1.741670	0.007634	0.703875
-41.735719	-1.916517	1.746675	0.007835	0.703632
-41.519403	-1.952758	1.751680	0.007794	0.703637
-41.837064	-1.900039	1.756685	0.007853	0.703629
-41.661373	-1.927144	1.761690	0.007821	0.703638
-41.340027	-1.985897	1.766694	0.007761	0.703635
-41.788733	-1.906686	1.771699	0.007844	0.703633
-41.446536	-1.964710	1.776704	0.007780	0.703640
-41.866486	-2.023112	1.781709	0.007859	0.703371
-42.257252	-1.967060	1.786714	0.007931	0.703343
-42.470446	-1.932303	1.791718	0.007971	0.703337
-42.596101	-1.909171	1.796723	0.007994	0.703339
-42.154681	-1.985773	1.801728	0.007912	0.703343
-42.452791	-1.936923	1.806733	0.007967	0.703335
-42.521113	-1.922426	1.811738	0.007980	0.703339
-43.300885	-1.950696	1.816742	0.008125	0.703002
-43.356720	-1.939238	1.821747	0.008135	0.703005
-43.249785	-1.958534	1.826752	0.008115	0.703005
-43.462442	-1.925763	1.831757	0.008155	0.702994
-43.481138	-1.918646	1.836762	0.008158	0.703002
-43.177360	-1.973071	1.841766	0.008102	0.703002
-43.217561	-1.964245	1.846771	0.008109	0.703005
-43.455270	-2.036508	1.851776	0.008153	0.702774
-44.475386	-1.897787	1.856781	0.008343	0.702687
-44.217591	-1.940618	1.861786	0.008295	0.702693
-43.977391	-1.983478	1.866790	0.008250	0.702693
-44.165963	-1.952102	1.871795	0.008285	0.702689
-44.081759	-1.965609	1.876800	0.008270	0.702692
-44.231845	-1.941133	1.881805	0.008297	0.702688
-44.426126	-2.038915	1.886810	0.008334	0.702420
-44.927529	-1.974965	1.891814	0.008427	0.702369
-45.329569	-1.904180	1.896819	0.008501	0.702367
-45.044340	-1.951094	1.901824	0.008448	0.702375
-45.099665	-1.945787	1.906829	0.008459	0.702366
-44.974146	-1.963996	1.911834	0.008435	0.702375
-45.385344	-1.893818	1.916838	0.008512	0.702369
-45.520623	-1.977440	1.921843	0.008537	0.702151
-45.927547	-1.940969	1.926848	0.008612	0.702078
-46.080212	-1.917727	1.931853	0.008641	0.702070
-46.089912	-1.913607	1.936858	0.008642	0.702075
-46.127752	-1.908676	1.941862	0.008649	0.702072
-45.946511	-1.942223	1.946867	0.008616	0.702069
-45.784508	-1.966785	1.951872	0.008585	0.702078
-46.031238	-2.027136	1.956877	0.008631	0.701867
-46.978784	-1.916939	1.961882	0.008808	0.701749
-46.915262	-1.931543	1.966886	0.008796	0.701742
-46.822529	-1.947421	1.971891	0.008778	0.701744
-46.857714	-1.939183	1.976896	0.008785	0.701748
-47.027248	-1.914165	1.981901	0.008816	0.701737
-46.784367	-1.952147	1.986906	0.008771	0.701748
-46.752352	-2.043369	1.991910	0.008765	0.701575
-48.058199	-1.879129	1.996915	0.009008	0.701437
-47.713671	-1.940398	2.001920	0.008944	0.701437

-47.591330	-1.962136	2.011917	0.008921	0.701438
-47.717129	-1.939093	2.021914	0.008944	0.701439
-47.610714	-1.959804	2.031910	0.008924	0.701436
-47.626174	-1.996796	2.041907	0.008927	0.701356
-48.031869	-1.952403	2.051904	0.009002	0.701299
-48.100132	-1.909445	2.061901	0.009015	0.701362
-47.802768	-1.924764	2.071898	0.008959	0.701439
-47.715154	-1.941814	2.081894	0.008943	0.701436
-47.647553	-1.954062	2.091891	0.008930	0.701436
-47.765530	-1.934189	2.101888	0.008952	0.701434
-47.490161	-1.981472	2.111885	0.008900	0.701438
-47.733343	-1.938890	2.121882	0.008945	0.701437
-47.822439	-1.922545	2.131878	0.008962	0.701438
-47.794014	-1.921982	2.141875	0.008956	0.701450
-47.025877	-1.914724	2.151872	0.008813	0.701742
-46.768430	-1.959312	2.161869	0.008765	0.701745
-46.882088	-1.939553	2.171866	0.008786	0.701744
-46.943565	-1.929059	2.181862	0.008797	0.701744
-46.253699	-1.968918	2.191859	0.008669	0.701912
-45.820567	-1.966770	2.201856	0.008588	0.702073
-45.856980	-1.960822	2.211853	0.008595	0.702072
-45.976755	-1.940321	2.221850	0.008617	0.702071
-45.742783	-1.955034	2.231846	0.008573	0.702126
-45.025604	-1.964625	2.241843	0.008439	0.702365
-44.952959	-1.976959	2.251840	0.008426	0.702367
-44.943662	-1.978619	2.261837	0.008424	0.702367
-45.037766	-1.908629	2.271834	0.008441	0.702475
-44.153155	-1.961613	2.281830	0.008276	0.702687
-44.260898	-1.944534	2.291827	0.008296	0.702683
-44.519888	-1.897400	2.301824	0.008344	0.702686
-43.591732	-1.923148	2.311821	0.008171	0.702968
-43.486177	-1.924020	2.321818	0.008151	0.703005
-43.298737	-1.958133	2.331814	0.008116	0.703004
-43.363878	-1.887259	2.341811	0.008128	0.703124
-42.375424	-1.958182	2.351808	0.007944	0.703337
-42.345955	-1.963514	2.361805	0.007938	0.703337
-42.471003	-1.941303	2.371802	0.007961	0.703337
-42.044069	-1.915654	2.381798	0.007882	0.703543
-41.556317	-1.961062	2.391795	0.007791	0.703627
-41.703193	-1.933024	2.401792	0.007818	0.703631
-41.196262	-2.007516	2.411789	0.007723	0.703663
-40.842685	-1.930549	2.421786	0.007657	0.703946
-40.555526	-1.981157	2.431782	0.007604	0.703948
-40.841082	-1.932233	2.441779	0.007657	0.703944
-40.460854	-1.910213	2.451776	0.007586	0.704125
-39.799782	-1.962915	2.461773	0.007463	0.704257
-39.840853	-1.956255	2.471770	0.007470	0.704256
-39.870558	-1.933097	2.481766	0.007475	0.704292
-39.038553	-1.936932	2.491763	0.007320	0.704584
-38.750342	-1.988268	2.501760	0.007267	0.704584
-38.602180	-2.015454	2.511757	0.007239	0.704583
-38.741281	-1.933469	2.521754	0.007265	0.704699
-37.898184	-1.993266	2.531750	0.007107	0.704881
-38.275333	-1.927130	2.541747	0.007177	0.704880
-37.890086	-1.995566	2.551744	0.007106	0.704880
-37.479612	-1.922389	2.561741	0.007029	0.705175
-37.179041	-1.959238	2.571738	0.006973	0.705209
-37.112585	-1.972909	2.581734	0.006960	0.705206
-37.025369	-1.917664	2.591731	0.006944	0.705349
-36.133300	-1.991530	2.601728	0.006778	0.705521
-36.202985	-1.979966	2.611725	0.006790	0.705519
-36.363629	-1.951180	2.621722	0.006820	0.705520
-35.585391	-1.936999	2.631718	0.006675	0.705828
-35.702047	-1.901953	2.641715	0.006697	0.705857
-35.245408	-1.982292	2.651712	0.006611	0.705859
-35.258258	-1.921032	2.661709	0.006614	0.705978
-34.425262	-1.996058	2.671706	0.006458	0.706126
-34.635890	-1.959453	2.681702	0.006497	0.706125
-34.842558	-1.910030	2.691699	0.006536	0.706150
-33.657641	-1.977121	2.701696	0.006315	0.706440
-33.886263	-1.936805	2.711693	0.006357	0.706440
-33.584838	-1.990138	2.721690	0.006301	0.706441
-33.313191	-1.944492	2.731686	0.006250	0.706630
-33.005268	-1.940294	2.741683	0.006193	0.706749
-32.725576	-1.990725	2.751680	0.006141	0.706748
-32.930463	-1.926672	2.761677	0.006179	0.706804
-31.991425	-1.955904	2.771674	0.006004	0.707082
-32.076700	-1.942654	2.781670	0.006019	0.707078
-32.074273	-1.943282	2.791667	0.006019	0.707078
-31.624651	-1.907581	2.801664	0.005935	0.707311
-31.517403	-1.895473	2.811661	0.005915	0.707374
-31.158828	-1.959259	2.821658	0.005848	0.707374
-31.012392	-1.897748	2.831654	0.005820	0.707551
-30.422124	-1.931395	2.841651	0.005710	0.707695
-30.350651	-1.944211	2.851648	0.005697	0.707695
-30.358266	-1.916445	2.861645	0.005698	0.707748
-29.535127	-1.933471	2.871642	0.005545	0.708008
-29.594137	-1.923229	2.881638	0.005555	0.708008
-29.476893	-1.945253	2.891635	0.005533	0.708006
-28.797114	-1.939876	2.901632	0.005407	0.708260
-28.657879	-1.921531	2.911629	0.005381	0.708347
-28.281870	-1.988926	2.921626	0.005310	0.708347
-28.432980	-1.959075	2.931622	0.005338	0.708353
-27.787614	-1.934002	2.941619	0.005218	0.708634
-27.666790	-1.955806	2.951616	0.005195	0.708633
-27.408197	-2.001224	2.961613	0.005147	0.708635
-27.554385	-1.903827	2.971610	0.005174	0.708778
-26.846308	-1.942718	2.981606	0.005042	0.708954
-27.126079	-1.894935	2.991603	0.005094	0.708950
-26.800937	-1.922824	3.001600	0.005033	0.709010
-26.048520	-1.930271	3.011597	0.004893	0.709264
-25.719779	-1.990567	3.021594	0.004832	0.709261
-26.059053	-1.929918	3.031590	0.004895	0.709262
-25.371553	-1.941137	3.041587	0.004767	0.709485
-25.091431	-1.937503	3.051584	0.004714	0.709592
-25.000150	-1.953026	3.061581	0.004697	0.709594
-24.937017	-1.956308	3.071578	0.004685	0.709610
-24.323953	-1.924348	3.081574	0.004571	0.709893
-24.321324	-1.926576	3.091571	0.004570	0.709890
-24.103082	-1.964329	3.101568	0.004529	0.709892
-23.915351	-1.903668	3.111565	0.004494	0.710081
-23.292336	-1.946615	3.121562	0.004378	0.710217
-23.407233	-1.928021	3.131558	0.004399	0.710214
-22.978826	-1.992233	3.141555	0.004319	0.710238
-22.706881	-1.895134	3.151552	0.004269	0.710529
-22.269180	-1.973042	3.161549	0.004187	0.710530
-22.240184	-1.977309	3.171546	0.004181	0.710532
-22.095318	-1.916041	3.181542	0.004154	0.710706
-21.373533	-1.965560	3.191539	0.004020	0.710865
-21.592661	-1.925932	3.201536	0.004060	0.710866
-21.130124	-2.007011	3.211533	0.003974	0.710869
-20.815694	-1.952578	3.221530	0.003915	0.711090
-20.662279	-1.958888	3.231526	0.003887	0.711132
-20.741643	-1.944396	3.241523	0.003901	0.711133
-20.498232	-1.929583	3.251520	0.003856	0.711250
-19.507491	-2.005293	3.261517	0.003671	0.711451
-19.809819	-1.950098	3.271514	0.003727	0.711454
-19.776489	-1.955958	3.281510	0.003721	0.711454
-19.004246	-1.959991	3.291507	0.003577	0.711721
-18.861881	-1.967525	3.301504	0.003550	0.711757
-18.588581	-2.014648	3.311501	0.003499	0.711760
-18.998663	-1.889508	3.321498	0.003575	0.711865
-17.885912	-1.974937	3.331494	0.003368	0.712090
-18.001672	-1.954236	3.341491	0.003389	0.712090
-18.029750	-1.949195	3.351488	0.003394	0.712091
-17.257050	-1.959648	3.361485	0.003250	0.712345
-17.200419	-1.950441	3.371482	0.003240	0.712383
-16.846343	-2.011754	3.381478	0.003174	0.712387
-16.950215	-1.954966	3.391475	0.003193	0.712464
-16.124407	-1.979437	3.401472	0.003039	0.712708
-15.941003	-2.011011	3.411469	0.003005	0.712711
-16.040000	-1.993767	3.421466	0.003023	0.712710
-15.831587	-1.948048	3.431462	0.002984	0.712876
-15.116927	-2.001482	3.441459	0.002851	0.713023
-15.111067	-2.002094	3.451456	0.002849	0.713024
-15.107918	-2.003047	3.461453	0.002849	0.713024
-14.589853	-1.953228	3.471450	0.002752	0.713307
-14.088044	-2.016814	3.481446	0.002658	0.713359
-14.159485	-2.005148	3.491443	0.002672	0.713357
-14.134696	-1.986899	3.501440	0.002667	0.713402
-13.286267	-2.011958	3.511437	0.002509	0.713653
-13.088997	-2.046627	3.521434	0.002472	0.713655
-13.330164	-2.005906	3.531430	0.002516	0.713650
-13.186992	-1.962794	3.541427	0.002490	0.713787
-12.075733	-2.068603	3.551424	0.002283	0.713971
-12.242997	-2.039280	3.561421	0.002314	0.713970
-12.527937	-1.986951	3.571418	0.002366	0.713973
-11.745009	-2.017850	3.581414	0.002220	0.714190
-11.566465	-2.007020	3.591411	0.002187	0.714275
-11.267396	-2.059701	3.601408	0.002131	0.714276
-11.073122	-2.094030	3.611405	0.002095	0.714277
-10.714809	-2.020048	3.621402	0.002028	0.714551
-10.476449	-2.033937	3.631398	0.001983	0.714608
-10.522182	-2.026105	3.641395	0.001992	0.714608
-10.158107	-2.078755	3.651392	0.001924	0.714632
-9.607581	-2.037282	3.661389	0.001821	0.714910
-9.442012	-2.066733	3.671386	0.001790	0.714910
-9.662850	-2.027988	3.681382	0.001831	0.714909
-9.514130	-1.975890	3.691379	0.001803	0.715065
-8.642216	-2.048645	3.701376	0.001641	0.715230
-8.491420	-2.073613	3.711373	0.001613	0.715234
-8.586384	-2.056737	3.721370	0.001630	0.715234
-7.724565	-2.078422	3.731366	0.001469	0.715496
-7.962335	-2.010736	3.741363	0.001514	0.715546
-7.663376	-2.063864	3.751360	0.001458	0.715547
-7.985734	-1.956757	3.761357	0.001518	0.715646
-6.791723	-2.048445	3.771354	0.001295	0.715886
-6.711584	-2.063230	3.781350	0.001280	0.715885
-7.001397	-2.012952	3.791347	0.001334	0.715883
-6.498139	-2.014696	3.801344	0.001240	0.716057
-6.151776	-2.039155	3.811341	0.001175	0.716131
-6.093311	-2.048344	3.821338	0.001164	0.716134
-6.069981	-1.992902	3.831334	0.001160	0.716252
-5.428437	-2.009636	3.841331	0.001040	0.716446
-5.296949	-2.032185	3.851328	0.001015	0.716448
-5.491069	-1.980013	3.861325	0.001051	0.716483
-4.412915	-2.033459	3.871322	0.000851	0.716758
-4.510033	-2.017820	3.881318	0.000868	0.716755
-4.484424	-2.022498	3.891315	0.000863	0.716755
-3.981839	-1.990756	3.901312	0.000770	0.716995
-3.521015	-2.028317	3.911309	0.000684	0.717084
-3.473556	-2.036807	3.921306	0.000675	0.717084
-3.404877	-2.021667	3.931302	0.000662	0.717138
-2.907209	-1.988386	3.941299	0.000569	0.717380
-2.518467	-2.057812	3.951296	0.000496	0.717380
-2.738985	-2.016880	3.961293	0.000537	0.717383
-2.427766	-1.949758	3.971290	0.000479	0.717626
-1.954024	-1.993409	3.981286	0.000391	0.717707
-2.218034	-1.945128	3.991283	0.000440	0.717710
-1.618413	-1.952753	4.001280	0.000328	0.717906
-1.451622	-1.923455	4.011277	0.000297	0.718023
-1.692257	-1.879929	4.021274	0.000341	0.718025
-1.306010	-1.833530	4.031270	0.000269	0.718252
-1.429362	-1.759182	4.041267	0.000292	0.718356
-1.299295	-1.753418	4.051264	0.000268	0.718414
-1.339678	-1.627025	4.061261	0.000275	0.718649
-1.320487	-1.614212	4.071258	0.000271	0.718682
-1.199950	-1.491442	4.081254	0.000248	0.718967
-1.149785	-1.470197	4.091251	0.000239	0.719027
-0.883786	-1.391325	4.101248	0.000189	0.719276
-1.092479	-1.285897	4.111245	0.000228	0.719411
-0.708194	-1.254811	4.121242	0.000156	0.719607
-0.825248	-1.126699	4.131238	0.000178	0.719819
-0.965389	-1.028510	4.141235	0.000203	0.719964
-0.703688	-0.941563	4.151232	0.000155	0.720227
-0.570982	-0.849773	4.161229	0.000130	0.720455
-0.836059	-0.699230	4.171226	0.000179	0.720659
-0.443695	-0.655823	4.181222	0.000105	0.720882
-0.691721	-0.489946	4.191219	0.000151	0.721122
-0.307793	-0.437810	4.201216	0.000080	0.721359
-0.257585	-0.327015	4.211213	0.000070	0.721595
-0.240950	-0.202371	4.221210	0.000067	0.721846
-0.279946	-0.053420	4.231206	0.000074	0.722126
-0.199014	0.064806	4.241203	0.000058	0.722386
0.000000	0.239641	4.251200	0.000021	0.722800

-0.060278	0.875860	4.256205	0.000032	0.724027
0.125781	2.107137	4.261210	-0.000004	0.726500
0.303589	3.932141	4.266214	-0.000038	0.730117
0.629453	6.285053	4.271219	-0.000100	0.734788
0.950019	9.151195	4.276224	-0.000162	0.740411
1.376171	12.478729	4.281229	-0.000244	0.746904
2.043325	16.225592	4.286234	-0.000370	0.754211
2.113901	20.473457	4.291238	-0.000386	0.762183
2.514834	25.067901	4.296243	-0.000464	0.770819
3.028770	30.007688	4.301248	-0.000563	0.780024
3.432974	35.314251	4.306253	-0.000642	0.789746
3.839122	40.946592	4.311258	-0.000721	0.799928
4.316143	46.857046	4.316262	-0.000814	0.810490
4.521033	53.103113	4.321267	-0.000856	0.821413
5.194104	59.539023	4.326272	-0.000986	0.832657
5.622152	66.234125	4.331277	-0.001070	0.844114
6.117073	73.152105	4.336282	-0.001167	0.855807
8.687907	79.906473	4.341286	-0.001650	0.867671
9.916492	87.127200	4.346291	-0.001884	0.879745
10.682438	94.614247	4.351296	-0.002031	0.891950
11.354369	102.256131	4.356301	-0.002161	0.904206
11.922939	110.080199	4.361306	-0.002272	0.916552
12.749460	117.961779	4.366310	-0.002431	0.928890
13.784233	125.943862	4.371315	-0.002629	0.941273
14.690089	134.062186	4.376320	-0.002803	0.953663
15.138364	142.322087	4.381325	-0.002892	0.965984
16.610644	150.506862	4.386330	-0.003172	0.978300
17.315076	158.904365	4.391334	-0.003309	0.990574
18.081008	167.322606	4.396339	-0.003457	1.002743
19.391764	175.702432	4.401344	-0.003706	1.014844
20.093693	184.220018	4.406349	-0.003843	1.026845
20.961785	192.772219	4.411354	-0.004010	1.038795
21.427888	201.398822	4.416358	-0.004103	1.050614
22.301467	209.987824	4.421363	-0.004271	1.062345
22.913825	218.655688	4.426368	-0.004391	1.073993
23.859871	227.231769	4.431373	-0.004572	1.085470
25.014053	235.820162	4.436378	-0.004793	1.096889
26.074373	244.418946	4.441382	-0.004996	1.108182
26.691270	253.116587	4.446387	-0.005117	1.119389
27.571915	261.747197	4.451392	-0.005286	1.130458
28.935727	270.309247	4.456397	-0.005546	1.141437
29.562661	279.035103	4.461402	-0.005669	1.152356
30.323977	287.669908	4.466406	-0.005816	1.163090
31.427596	296.251056	4.471411	-0.006027	1.173731
31.766900	304.937165	4.476416	-0.006096	1.184245
32.432262	313.560719	4.481421	-0.006226	1.194659
33.341206	322.133787	4.486426	-0.006401	1.204971
33.968150	330.736965	4.491430	-0.006523	1.215175
34.676683	339.316708	4.496435	-0.006661	1.225282
35.433866	347.901069	4.501440	-0.006807	1.235321
36.295294	356.401677	4.506445	-0.006973	1.245203
37.260742	364.916522	4.511450	-0.007159	1.255043
37.715686	373.469749	4.516454	-0.007249	1.264753
38.378818	382.005260	4.521459	-0.007378	1.274408
39.159907	390.484938	4.526464	-0.007529	1.283950
39.597377	399.016322	4.531469	-0.007616	1.293414
40.382694	407.479932	4.536474	-0.007768	1.302800
40.846413	416.058822	4.541478	-0.007860	1.312184
41.511773	424.537972	4.546483	-0.007990	1.321430
42.172123	432.951370	4.551488	-0.008118	1.330542
42.837898	441.343707	4.556493	-0.008248	1.339569
43.368841	449.770146	4.561498	-0.008352	1.348548
43.510710	458.232217	4.566502	-0.008384	1.357437
44.543962	466.523439	4.571507	-0.008582	1.366244
45.252851	474.911660	4.576512	-0.008720	1.375040
45.591743	483.304802	4.581517	-0.008788	1.383721
46.267972	491.688413	4.586522	-0.008920	1.392395
46.862381	500.028620	4.591526	-0.009036	1.400957
47.443237	508.370584	4.596531	-0.009150	1.409467
47.806030	516.758701	4.601536	-0.009223	1.417935
48.539071	525.043770	4.606541	-0.009365	1.426311
49.040376	533.399642	4.611546	-0.009464	1.434671
49.326018	541.739932	4.616550	-0.009522	1.442931
49.813866	550.059604	4.621555	-0.009619	1.451157
50.419633	558.352727	4.626560	-0.009737	1.459329
51.094429	566.624687	4.631565	-0.009868	1.467446
51.532503	575.002211	4.636570	-0.009955	1.475582
52.113090	583.253605	4.641574	-0.010069	1.483575
52.487431	591.553315	4.646579	-0.010144	1.491539
52.858084	599.851472	4.651584	-0.010218	1.499459
53.471758	608.083362	4.656589	-0.010338	1.507311
53.816385	616.397832	4.661594	-0.010408	1.515159
54.263088	624.647207	4.666598	-0.010496	1.522921
55.045037	632.852135	4.671603	-0.010647	1.530653
55.390454	641.141076	4.676608	-0.010717	1.538358
55.845495	649.366245	4.681613	-0.010807	1.545983
56.525642	657.621207	4.686618	-0.010940	1.553630
57.224509	665.810292	4.691622	-0.011075	1.561182
57.850117	674.031878	4.696627	-0.011197	1.568716
58.583156	682.249213	4.701632	-0.011339	1.576226
58.944502	690.494088	4.706637	-0.011412	1.583671
59.542347	698.728473	4.711642	-0.011528	1.591106
59.757665	706.995040	4.716646	-0.011574	1.598479
60.443234	715.170873	4.721651	-0.011707	1.605806
60.757072	723.433767	4.726656	-0.011771	1.613123
61.255373	731.630621	4.731661	-0.011869	1.620375
61.648177	739.875215	4.736666	-0.011948	1.627621
62.026412	748.145140	4.741670	-0.012024	1.634855
62.459712	756.320530	4.746675	-0.012110	1.641983
62.815959	764.519524	4.751680	-0.012182	1.649090
63.086224	772.727480	4.756685	-0.012237	1.656162
63.772892	780.883121	4.761690	-0.012371	1.663216
64.334086	789.045294	4.766694	-0.012480	1.670228
64.928678	797.224008	4.771699	-0.012597	1.677229
65.663356	805.371615	4.776704	-0.012739	1.684194
65.985183	813.580600	4.781709	-0.012804	1.691126
66.406438	821.798985	4.786714	-0.012888	1.698051
66.752014	829.970319	4.791718	-0.012958	1.704898
67.349113	838.154945	4.796723	-0.013074	1.711762
67.693489	846.360528	4.801728	-0.013144	1.718583
68.124380	854.488735	4.806733	-0.013229	1.725324
68.620041	862.671129	4.811738	-0.013327	1.732091
68.853847	870.854050	4.816742	-0.013376	1.738799
69.162160	879.018527	4.821747	-0.013439	1.745476
69.964834	887.146293	4.826752	-0.013594	1.752159
70.188239	895.330953	4.831757	-0.013641	1.758791
70.829096	903.451963	4.836762	-0.013765	1.765398
71.143439	911.637676	4.841766	-0.013829	1.771991
71.570517	919.802009	4.846771	-0.013914	1.778557
72.103872	927.933448	4.851776	-0.014019	1.785086
72.531250	936.129802	4.856781	-0.014104	1.791629
72.932635	944.312229	4.861786	-0.014184	1.798134
73.366817	952.424751	4.866790	-0.014270	1.804564
73.888613	960.542753	4.871795	-0.014373	1.810986
74.355019	968.698239	4.876800	-0.014465	1.817408
74.512481	976.857434	4.881805	-0.014500	1.823773
74.889436	985.011967	4.886810	-0.014575	1.830139
75.378117	993.137426	4.891814	-0.014672	1.836473
75.786590	1001.256190	4.896819	-0.014753	1.842770
76.143961	1009.410759	4.901824	-0.014825	1.849068
76.576651	1017.545356	4.906829	-0.014911	1.855337
76.770053	1025.718799	4.911834	-0.014953	1.861587
77.432003	1033.812806	4.916838	-0.015081	1.867810
77.597885	1042.017671	4.921843	-0.015118	1.874039
77.971072	1050.126016	4.926848	-0.015192	1.880198
78.289666	1058.233008	4.931853	-0.015257	1.886330
78.781263	1066.369435	4.936858	-0.015354	1.892483
79.332649	1074.461580	4.941862	-0.015462	1.898590
79.862000	1082.561793	4.946867	-0.015566	1.904681
80.492844	1090.684251	4.951872	-0.015689	1.910779
80.735639	1098.828854	4.956877	-0.015739	1.916832
81.332565	1106.930142	4.961882	-0.015856	1.922873
81.583315	1115.066195	4.966886	-0.015908	1.928882
81.787997	1123.227964	4.971891	-0.015951	1.934886
82.392124	1131.311428	4.976896	-0.016069	1.940857
82.666449	1139.444899	4.981901	-0.016126	1.946811
83.080920	1147.605147	4.986906	-0.016208	1.952782
83.291047	1155.736221	4.991910	-0.016253	1.958690
83.725643	1163.807179	4.996915	-0.016339	1.964562
84.218705	1171.904816	5.001920	-0.016436	1.970441
84.647867	1180.012410	5.006925	-0.016522	1.976304
85.083422	1188.116408	5.011930	-0.016608	1.982146
85.293922	1196.240223	5.016934	-0.016653	1.987962
85.368747	1204.407060	5.021939	-0.016672	1.993777
85.982726	1212.467874	5.026944	-0.016792	1.999557
86.420054	1220.534679	5.031949	-0.016878	2.005305
86.668134	1228.679595	5.036954	-0.016930	2.011073
86.902157	1236.804378	5.041958	-0.016979	2.016808
87.524754	1244.855748	5.046963	-0.017100	2.022515
87.721701	1253.004676	5.051968	-0.017142	2.028231
88.064416	1261.126858	5.056973	-0.017211	2.033927
88.609957	1269.195548	5.061978	-0.017318	2.039590
88.869805	1277.290213	5.066982	-0.017372	2.045227
89.055133	1285.405456	5.071987	-0.017412	2.050854
89.371853	1293.529616	5.076992	-0.017476	2.056486
89.691374	1301.613144	5.081997	-0.017541	2.062074
89.911417	1309.742499	5.087002	-0.017588	2.067669
90.451452	1317.806773	5.092006	-0.017693	2.073235
90.883042	1325.885092	5.097011	-0.017779	2.078786
91.412632	1333.954350	5.102016	-0.017883	2.084325
91.428688	1342.104305	5.107021	-0.017891	2.089854
92.069358	1350.192582	5.112026	-0.018016	2.095387
92.386498	1358.275400	5.117030	-0.018080	2.100871
92.951070	1366.329694	5.122035	-0.018191	2.106345
93.376125	1374.474663	5.127040	-0.018275	2.111852
93.743357	1382.577874	5.132045	-0.018349	2.117311
94.170006	1390.642010	5.137050	-0.018434	2.122735
94.441793	1398.716497	5.142054	-0.018490	2.128138
94.892816	1406.805787	5.147059	-0.018579	2.133553
95.204741	1414.909491	5.152064	-0.018643	2.138952
95.305485	1422.997428	5.157069	-0.018667	2.144306
95.812172	1431.072113	5.162074	-0.018767	2.149676
96.068575	1439.190965	5.167078	-0.018820	2.155039
96.330599	1447.261058	5.172083	-0.018874	2.160356
96.691849	1455.350032	5.177088	-0.018946	2.165682
97.177555	1463.397223	5.182093	-0.019042	2.170979
97.744479	1471.488696	5.187098	-0.019153	2.176300
98.026557	1479.571929	5.192102	-0.019211	2.181575
98.217253	1487.680401	5.197107	-0.019252	2.186846
98.611612	1495.791432	5.202112	-0.019331	2.192125
98.664205	1503.904838	5.207117	-0.019346	2.197361
98.991763	1511.969520	5.212122	-0.019412	2.202578
99.219097	1520.040642	5.217126	-0.019460	2.207778
99.516691	1528.120126	5.222131	-0.019521	2.212977
99.780562	1536.201306	5.227136	-0.019575	2.218162
100.135103	1544.242055	5.232141	-0.019646	2.223317
100.583409	1552.325744	5.237146	-0.019735	2.228496
100.913466	1560.426856	5.242150	-0.019802	2.233663
101.345730	1568.475178	5.247155	-0.019888	2.238794
101.849627	1576.527608	5.252160	-0.019987	2.243922
102.379460	1584.568428	5.257165	-0.020091	2.249033
102.697502	1592.696636	5.262170	-0.020156	2.254169
103.109861	1600.767981	5.267174	-0.020238	2.259265
103.455967	1608.831059	5.272179	-0.020307	2.264339
103.440067	1616.973556	5.277184	-0.020310	2.269420
103.640108	1625.142128	5.282189	-0.020353	2.274524
104.008364	1633.167936	5.287194	-0.020426	2.279543
104.352573	1641.200395	5.292198	-0.020496	2.284553
104.813308	1649.237747	5.297203	-0.020587	2.289564
105.168687	1657.342192	5.302208	-0.020658	2.294597
105.320959	1665.402973	5.307213	-0.020692	2.299575
105.548584	1673.482465	5.312218	-0.020740	2.304559
105.964456	1681.524838	5.317222	-0.020823	2.309526
106.208035	1689.619578	5.322227	-0.020873	2.314500
106.518629	1697.684647	5.327232	-0.020937	2.319451
106.776950	1705.727097	5.332237	-0.020990	2.324372
107.252962	1713.782383	5.337242	-0.021084	2.329310
107.632352	1721.871817	5.342246	-0.021160	2.334249
107.688536	1729.947349	5.347251	-0.021176	2.339143
108.157117	1738.014559	5.352256	-0.021268	2.344055
108.270971	1746.095634	5.357261	-0.021295	2.348937
108.756826	1754.193805	5.362266	-0.021391	2.353848
109.073623	1762.232586	5.367270	-0.021455	2.358700
109.270687	1770.284170	5.372275	-0.021497	2.363540
109.378875	1778.372703	5.377280	-0.021523	2.368385
109.488262	1786.468558	5.382285	-0.021548	2.373225
110.073386	1794.492903	5.387290	-0.021662	2.378050
110.254089	1802.559635	5.392294	-0.021701	2.382858
110.492360	1810.629044	5.397299	-0.021751	2.387663
110.772902	1818.717162	5.402304	-0.021809	2.392472
111.040312	1826.767683	5.407309	-0.021864	2.397248
111.219104	1834.826614	5.412314	-0.021903	2.402013
111.566798	1842.877396	5.417318	-0.021973	2.406777
111.916408	1850.945978	5.422323	-0.022043	2.411542
112.481267	1858.994803	5.427328	-0.022154	2.416302
112.681378	1867.047974	5.432333	-0.022196	2.421027
113.042125	1875.104656	5.437338	-0.022269	2.425758
113.210126	1883.222557	5.442342	-0.022305	2.430500
113.480234	1891.348106	5.447347	-0.022361	2.435245
114.000604	1899.353416	5.452352	-0.022463	2.439930
114.286832	1907.371717	5.457357	-0.022522	2.444596
114.481011	1915.454350	5.462362	-0.022563	2.449283
114.646742	1923.528426	5.467366	-0.022599	2.453953
114.716949	1931.600087	5.472371	-0.022618	2.458607
115.020738	1939.642505	5.477376	-0.022680	2.463252
115.427025	1947.678250	5.482381	-0.022761	2.467892
115.892829	1955.756855	5.487386	-0.022853	2.472553
116.175641	1963.815708	5.492390	-0.022911	2.477179
116.331557	1971.861068	5.497395	-0.022945	2.481780
116.650431	1979.912456	5.502400	-0.023010	2.486388
117.010775	1987.968135	5.507405	-0.023082	2.490992
117.173053	1996.070570	5.512410	-0.023118	2.495601
117.504618	2004.096474	5.517414	-0.023185	2.500169
117.791003	2012.133689	5.522419	-0.023244	2.504732
118.211086	2020.198772	5.527424	-0.023327	2.509313
118.538677	2028.289614	5.532429	-0.023393	2.513892
118.917467	2036.337170	5.537434	-0.023469	2.518443
118.974532	2044.379943	5.542438	-0.023485	2.522960
119.264317	2052.415285	5.547443	-0.023545	2.527481
119.768396	2060.475349	5.552448	-0.023644	2.532022
119.915267	2068.548619	5.557453	-0.023676	2.536538
120.209257	2076.594970	5.562458	-0.023737	2.541041
120.681310	2084.609600	5.567462	-0.023830	2.545531
121.001009	2092.672331	5.572467	-0.023895	2.550029
121.399212	2100.750013	5.577472	-0.023974	2.554533
121.650782	2108.782753	5.582477	-0.024026	2.558993
122.087814	2116.825823	5.587482	-0.024113	2.563464
122.204463	2124.910776	5.592486	-0.024140	2.567929
122.536471	2132.956129	5.597491	-0.024207	2.572378
122.852640	2141.039231	5.602496	-0.024271	2.576840
123.234290	2149.081897	5.607501	-0.024348	2.581276
123.410658	2157.129490	5.612506	-0.024386	2.585693
123.773981	2165.187346	5.617510	-0.024459	2.590121
123.987692	2173.441705	5.622515	-0.024504	2.594638
124.136288	2181.452722	5.627520	-0.024537	2.599010
124.171260	2189.452649	5.632525	-0.024549	2.603361
124.412420	2197.469484	5.637530	-0.024599	2.607729
124.704376	2205.494485	5.642534	-0.024659	2.612096
124.907054	2213.547610	5.647539	-0.024702	2.616465
125.394750	2221.558013	5.652544	-0.024798	2.620823
125.539544	2229.580852	5.657549	-0.024830	2.625158
125.959550	2237.630490	5.662554	-0.024914	2.629518
126.107766	2245.716099	5.667558	-0.024947	2.633872
126.426494	2253.741840	5.672563	-0.025011	2.638198
126.707680	2261.778841	5.677568	-0.025069	2.642521
126.688987	2269.823189	5.682573	-0.025071	2.646820
127.031464	2277.890078	5.687578	-0.025140	2.651148
127.441204	2285.953662	5.692582	-0.025222	2.655472
127.682622	2293.978888	5.697587	-0.025272	2.659757
127.912551	2302.042134	5.702592	-0.025320	2.664055
128.273042	2310.070891	5.707597	-0.025393	2.668336
128.412236	2318.174382	5.712602	-0.025424	2.672635
128.398327	2326.266376	5.717606	-0.025427	2.676912
128.591251	2334.254576	5.722611	-0.025468	2.681140
129.027836	2342.279508	5.727616	-0.025554	2.685396
129.157337	2350.311623	5.732621	-0.025584	2.689630
129.648752	2358.378437	5.737626	-0.025681	2.693898
130.005147	2366.406016	5.742630	-0.025752	2.698130
130.348103	2374.418187	5.747635	-0.025821	2.702347
130.666679	2382.480062	5.752640	-0.025886	2.706581
131.131942	2390.495946	5.757645	-0.025978	2.710794
131.397303	2398.600557	5.762650	-0.026033	2.715034
131.546618	2406.641729	5.767654	-0.026066	2.719227
131.702468	2414.675988	5.772659	-0.026100	2.723411
132.156987	2422.711384	5.777664	-0.026190	2.727607
132.283609	2430.772895	5.782669	-0.026219	2.731789
132.520313	2438.846525	5.787674	-0.026269	2.735979
132.909065	2446.858462	5.792678	-0.026346	2.740139
132.907223	2454.912440	5.797683	-0.026351	2.744291
133.174788	2463.000971	5.802688	-0.026406	2.748471
133.232560	2471.088910	5.807693	-0.026423	2.752631
133.616551	2479.139944	5.812698	-0.026499	2.756786
133.717868	2487.166907	5.817702	-0.026524	2.760905
133.995173	2495.148732	5.822707	-0.026580	2.765006
134.441979	2503.194975	5.827712	-0.026669	2.769143
134.688412	2511.235797	5.832717	-0.026720	2.773259
134.881046	2519.288219	5.837722	-0.026761	2.777372
135.134393	2527.325994	5.842726	-0.026814	2.781475
135.358380	2535.346581	5.847731	-0.026861	2.785562
135.635258	2543.405622	5.852736	-0.026918	2.789665
135.725175	2551.478522	5.857741	-0.026940	2.793757
136.206494	2559.484242	5.862746	-0.027035	2.797833
136.409025	2567.519744	5.867750	-0.027078	2.801902
136.438714	2575.565820	5.872755	-0.027089	2.805960
136.813167	2583.621292	5.877760	-0.027164	2.810037
137.146986	2591.654173	5.882765	-0.027231	2.814094
137.634473	2599.679421	5.887770	-0.027327	2.818150
137.803275	2607.725422	5.892774	-0.027364	2.822192
138.021768	2615.784896	5.897779	-0.027410	2.826238
138.366300	2623.826100	5.902784	-0.027480	2.830276
138.659819	2631.891035	5.907789	-0.027540	2.834318
138.954916	2639.943023	5.912794	-0.027600	2.838347
139.176432	2647.947138	5.917798	-0.027646	2.842343
139.397974	2655.970186	5.922803	-0.027693	2.846342
140.010936	2664.007148	5.927808	-0.027812	2.850364
140.128380	2672.089463	5.932813	-0.027840	2.854376
140.301579	2680.125820	5.937818	-0.027877	2.858362
140.621260	2688.148866	5.942822	-0.027942	2.862344
140.791275	2696.203807	5.947827	-0.027979	2.866328
140.983871	2704.248515	5.952832	-0.028020	2.870303
140.890967	2712.335040	5.957837	-0.028008	2.874277
141.332640	2720.339536	5.962842	-0.028096	2.878234
141.537611	2728.377769	5.967846	-0.028139	2.882190
141.852907	2736.377316	5.972851	-0.028203	2.886127
142.211631	2744.427850	5.977856	-0.028275	2.890086
142.123237	2752.524960	5.982861	-0.028264	2.894038
142.448492	2760.523461	5.987866	-0.028330	2.897959
142.977512	2768.549651	5.992870	-0.028434	2.901899
143.050904	2776.587044	5.997875	-0.028453	2.905815
143.381789	2784.646291	6.002880	-0.028520	2.909749
143.578529	2792.753207	6.007885	-0.028562	2.913695
143.933683	2800.779790	6.012890	-0.028633	2.917604
144.107298	2808.786803	6.017894	-0.028671	2.921489
143.940075	2816.834585	6.022899	-0.028645	2.925370
144.282693	2824.838844	6.027904	-0.028714	2.929253
144.570190	2832.868966	6.032909	-0.028773	2.933139
144.728205	2840.920682	6.037914	-0.028808	2.937024
144.991302	2848.953599	6.042918	-0.028862	2.940901
145.192500	2856.950597	6.047923	-0.028905	2.944751
145.476102	2865.019653	6.052928	-0.028963	2.948636
145.649196	2873.082040	6.057933	-0.029001	2.952506
146.042804	2881.113803	6.062938	-0.029079	2.956368
146.312827	2889.102819	6.067942	-0.029135	2.960198
146.475322	2897.143300	6.072947	-0.029170	2.964042
146.964711	2905.186304	6.077952	-0.029267	2.967899
147.108103	2913.239479	6.082957	-0.029299	2.971738
147.279929	2921.293555	6.087962	-0.029336	2.975574
147.775909	2929.298699	6.092966	-0.029434	2.979398
148.008502	2937.308031	6.097971	-0.029482	2.983206
148.228974	2945.378507	6.102976	-0.029529	2.987038
148.372056	2953.422704	6.107981	-0.029561	2.990848
148.653031	2961.516306	6.112986	-0.029618	2.994683
148.930184	2969.511530	6.117990	-0.029675	2.998467
149.158645	2977.518801	6.122995	-0.029723	3.002249
149.414574	2985.559986	6.128000	-0.029776	3.006044
149.746998	2993.564903	6.133005	-0.029843	3.009821
149.733245	3001.668795	6.138010	-0.029846	3.013622
150.001422	3009.683542	6.143014	-0.029901	3.017391
150.332601	3017.711251	6.148019	-0.029968	3.021164
150.567884	3025.730389	6.153024	-0.030018	3.024923
150.920060	3033.758231	6.158029	-0.030088	3.028688
151.487698	3041.810159	6.163034	-0.030199	3.032469
151.758160	3049.879629	6.168038	-0.030255	3.036239
151.998597	3057.871016	6.173043	-0.030305	3.039967
152.104138	3065.937327	6.178048	-0.030330	3.043719
152.341684	3073.938829	6.183053	-0.030380	3.047442
152.359214	3082.011885	6.188058	-0.030388	3.051184
152.657514	3090.062117	6.193062	-0.030449	3.054923
153.083509	3098.054602	6.198067	-0.030534	3.058638
153.175778	3106.103192	6.203072	-0.030556	3.062357
153.312034	3114.117856	6.208077	-0.030587	3.066059
153.505136	3122.171113	6.213082	-0.030628	3.069777
154.057378	3130.258331	6.218086	-0.030736	3.073522
154.108470	3138.315900	6.223091	-0.030751	3.077226
154.450398	3146.315077	6.228096	-0.030820	3.080912
154.651017	3154.298021	6.233101	-0.030863	3.084580
154.913067	3162.326718	6.238106	-0.030917	3.088267
155.091488	3170.383102	6.243110	-0.030956	3.091959
155.154831	3178.428574	6.248115	-0.030973	3.095635
155.601607	3186.449473	6.253120	-0.031061	3.099314
155.650911	3194.464205	6.258125	-0.031076	3.102967
155.986833	3202.499040	6.263130	-0.031144	3.106639
156.301574	3210.529851	6.268134	-0.031207	3.110303
156.420734	3218.586236	6.273139	-0.031235	3.113965
156.795871	3226.595860	6.278144	-0.031310	3.117613
156.674309	3234.651662	6.283149	-0.031293	3.121256
156.929473	3242.664526	6.288154	-0.031346	3.124892
157.271251	3250.691484	6.293158	-0.031415	3.128534
157.437987	3258.747914	6.298163	-0.031451	3.132177
157.853499	3266.786691	6.303168	-0.031534	3.135819
157.824876	3274.812506	6.308173	-0.031534	3.139431
157.972051	3282.840143	6.313178	-0.031566	3.143047
158.313461	3290.863771	6.318182	-0.031635	3.146666
158.608605	3298.887384	6.323187	-0.031696	3.150279
158.952136	3306.967257	6.328192	-0.031765	3.153915
159.495940	3314.946545	6.333197	-0.031871	3.157510
159.476753	3322.974873	6.338202	-0.031873	3.161099
159.986575	3330.969763	6.343206	-0.031973	3.164692
160.161028	3339.006937	6.348211	-0.032011	3.168284
160.392462	3347.089226	6.353216	-0.032060	3.171896
160.594046	3355.110714	6.358221	-0.032102	3.175474
160.840450	3363.156049	6.363226	-0.032154	3.179062
161.151373	3371.181238	6.368230	-0.032217	3.182639
161.284480	3379.208590	6.373235	-0.032247	3.186205
161.416717	3387.256373	6.378240	-0.032277	3.189776
161.887867	3395.278315	6.383245	-0.032370	3.193346
162.131385	3403.332413	6.388250	-0.032421	3.196917
162.453886	3411.335843	6.393254	-0.032486	3.200464
162.381591	3419.372744	6.398259	-0.032478	3.204006
162.825625	3427.406156	6.403264	-0.032566	3.207564
163.078774	3435.433254	6.408269	-0.032618	3.211107
163.272934	3443.479843	6.413274	-0.032660	3.214652
163.590576	3451.508952	6.418278	-0.032724	3.218191
163.487721	3459.553483	6.423283	-0.032710	3.221716
163.879718	3467.566474	6.428288	-0.032789	3.225243
164.148668	3475.584866	6.433293	-0.032844	3.228763
164.140566	3483.683526	6.438298	-0.032848	3.232303
164.394329	3491.741127	6.443302	-0.032900	3.235832
164.572386	3499.702931	6.448307	-0.032939	3.239313
165.020676	3507.736704	6.453312	-0.033028	3.242832
165.067383	3515.740945	6.458317	-0.033042	3.246318
165.484206	3523.712015	6.463322	-0.033125	3.249800
165.547213	3531.823432	6.468326	-0.033142	3.253326
165.909851	3539.822765	6.473331	-0.033214	3.256811
166.112752	3547.872056	6.478336	-0.033258	3.260308
166.407386	3555.861881	6.483341	-0.033318	3.263778
166.653710	3563.900130	6.488346	-0.033369	3.267264
166.918182	3571.951959	6.493350	-0.033424	3.270753
167.177876	3579.987620	6.498355	-0.033477	3.274231
167.333793	3588.028983	6.503360	-0.033512	3.277704
167.574579	3596.032889	6.508365	-0.033562	3.281160
167.958536	3603.996219	6.513370	-0.033638	3.284600
168.251419	3612.063467	6.518374	-0.033698	3.288078
168.424513	3620.110801	6.523379	-0.033736	3.291539
168.684375	3628.173540	6.528384	-0.033790	3.295007
168.764523	3636.182117	6.533389	-0.033810	3.298440
169.413911	3644.182202	6.538394	-0.033936	3.301888
169.840589	3652.193133	6.543398	-0.034021	3.305329
169.798352	3660.261323	6.548403	-0.034018	3.308772
170.258033	3668.307623	6.553408	-0.034109	3.312222
170.645652	3676.343949	6.558413	-0.034187	3.315660
170.758201	3684.354220	6.563418	-0.034213	3.319074
170.973546	3692.381439	6.568422	-0.034258	3.322496
171.098795	3700.382256	6.573427	-0.034287	3.325899
171.524502	3708.419646	6.578432	-0.034372	3.329326
171.610950	3716.461842	6.583437	-0.034393	3.332738
171.918902	3724.497557	6.588442	-0.034456	3.336152
172.173103	3732.508650	6.593446	-0.034508	3.339550
172.129052	3740.541202	6.598451	-0.034505	3.342943
172.426140	3748.593227	6.603456	-0.034566	3.346354
172.542774	3756.611345	6.608461	-0.034593	3.349739
172.736297	3764.675533	6.613466	-0.034634	3.353144
172.907622	3772.723198	6.618470	-0.034672	3.356537
173.202939	3780.678628	6.623475	-0.034732	3.359893
173.405014	3788.720742	6.628480	-0.034775	3.363278
173.410325	3796.752037	6.633485	-0.034781	3.366648
173.889320	3804.740830	6.638490	-0.034876	3.370014
174.178086	3812.827769	6.643494	-0.034935	3.373411
174.331894	3820.842544	6.648499	-0.034969	3.376769
174.694199	3828.850829	6.653504	-0.035041	3.380129
175.130591	3836.840844	6.658509	-0.035128	3.383480
175.282520	3844.902504	6.663514	-0.035162	3.386847
175.484898	3852.951563	6.668518	-0.035205	3.390208
175.723669	3861.037196	6.673523	-0.035254	3.393582
176.094306	3869.086233	6.678528	-0.035329	3.396942
176.258688	3877.055264	6.683533	-0.035365	3.400258
176.269055	3885.049419	6.688538	-0.035372	3.403576
176.414180	3893.101285	6.693542	-0.035404	3.406920
176.510609	3901.106327	6.698547	-0.035427	3.410239
177.010183	3909.139693	6.703552	-0.035526	3.413580
177.087327	3917.171972	6.708557	-0.035546	3.416903
177.317200	3925.176180	6.713562	-0.035594	3.420216
177.667390	3933.191321	6.718566	-0.035664	3.423535
177.889902	3941.210404	6.723571	-0.035711	3.426848
178.247885	3949.248359	6.728576	-0.035783	3.430170
178.367219	3957.296144	6.733581	-0.035810	3.433484
178.434524	3965.336212	6.738586	-0.035828	3.436791
178.724197	3973.347123	6.743590	-0.035887	3.440089
178.662089	3981.366732	6.748595	-0.035881	3.443377
178.920933	3989.383490	6.753600	-0.035935	3.446671
179.308387	3997.410727	6.758605	-0.036012	3.449970
179.421120	4005.469287	6.763610	-0.036039	3.453269
179.602171	4013.530177	6.768614	-0.036078	3.456569
179.857318	4021.484325	6.773619	-0.036130	3.459824
180.046419	4029.565439	6.778624	-0.036171	3.463126
180.261453	4037.576418	6.783629	-0.036216	3.466397
180.381807	4045.598696	6.788634	-0.036244	3.469666
180.668521	4053.661609	6.793638	-0.036303	3.472954
180.641641	4061.706158	6.798643	-0.036303	3.476222
181.036133	4069.683753	6.803648	-0.036382	3.479473
181.138879	4077.687913	6.808653	-0.036406	3.482722
181.149570	4085.701370	6.813658	-0.036413	3.485969
181.337481	4093.714726	6.818662	-0.036454	3.489218
181.676065	4101.771094	6.823667	-0.036522	3.492486
181.892186	4109.812163	6.828672	-0.036568	3.495742
181.900172	4117.842821	6.833677	-0.036574	3.498983
182.081205	4125.845175	6.838682	-0.036613	3.502216
182.384344	4133.848755	6.843686	-0.036675	3.505450
182.413674	4141.877704	6.848691	-0.036686	3.508682
182.695857	4149.910330	6.853696	-0.036744	3.511921
183.050223	4157.945018	6.858701	-0.036815	3.515160
183.275319	4165.966746	6.863706	-0.036862	3.518386
183.529390	4174.014788	6.868710	-0.036915	3.521621
183.614322	4181.955263	6.873715	-0.036936	3.524805
183.772162	4190.045737	6.878720	-0.036971	3.528048
183.900419	4198.088941	6.883725	-0.037000	3.531269
184.322321	4206.105836	6.888730	-0.037084	3.534484
184.526942	4214.154288	6.893734	-0.037127	3.537703
184.498498	4222.162529	6.898739	-0.037127	3.540896
184.820122	4230.188042	6.903744	-0.037193	3.544103
185.125181	4238.212007	6.908749	-0.037255	3.547306
185.171973	4246.214555	6.913754	-0.037269	3.550490
185.635416	4254.353959	6.918758	-0.037360	3.553738
185.817924	4262.365114	6.923763	-0.037400	3.556924
185.926592	4270.335408	6.928768	-0.037425	3.560088
185.931111	4278.364603	6.933773	-0.037431	3.563270
186.364455	4286.346046	6.938778	-0.037517	3.566443
186.834261	4294.343994	6.943782	-0.037610	3.569620
186.729328	4302.428120	6.948787	-0.037596	3.572812
186.820383	4310.460171	6.953792	-0.037618	3.575986
187.025807	4318.447612	6.958797	-0.037662	3.579143
187.288325	4326.484851	6.963802	-0.037716	3.582319
187.383791	4334.503265	6.968806	-0.037739	3.585479
187.496916	4342.491024	6.973811	-0.037765	3.588625
187.857143	4350.569125	6.978816	-0.037838	3.591811
188.037696	4358.577493	6.983821	-0.037877	3.594961
188.167322	4366.596588	6.988826	-0.037906	3.598112
188.436201	4374.601771	6.993830	-0.037961	3.601258
188.620303	4382.561860	6.998835	-0.038001	3.604381
188.690138	4390.646316	7.003840	-0.038019	3.607547
189.052379	4398.661482	7.008845	-0.038092	3.610691
189.418475	4406.713117	7.013850	-0.038166	3.613847
189.436238	4414.768264	7.018854	-0.038174	3.616992
189.581577	4422.747882	7.023859	-0.038207	3.620108
189.867521	4430.757555	7.028864	-0.038265	3.623236
190.053461	4438.787626	7.033869	-0.038305	3.626368
190.116059	4446.802727	7.038874	-0.038322	3.629487
190.560973	4454.891679	7.043878	-0.038410	3.632643
190.710778	4462.934924	7.048883	-0.038443	3.635770
190.979506	4470.931148	7.053888	-0.038499	3.638880
191.249794	4478.934233	7.058893	-0.038554	3.641989
191.591326	4486.896702	7.063898	-0.038623	3.645082
191.901328	4494.941679	7.068902	-0.038686	3.648204
191.816677	4502.987260	7.073907	-0.038676	3.651312
192.297575	4511.034684	7.078912	-0.038771	3.654434
192.505038	4519.060662	7.083917	-0.038815	3.657537
192.417492	4527.087414	7.088922	-0.038804	3.660630
192.743803	4535.113529	7.093926	-0.038870	3.663731
192.685346	4543.134108	7.098931	-0.038864	3.666818
193.000317	4551.147983	7.103936	-0.038928	3.669909
193.097900	4559.205104	7.108941	-0.038952	3.673008
193.483175	4567.211041	7.113946	-0.039029	3.676092
193.651108	4575.221099	7.118950	-0.039065	3.679170
193.780757	4583.229869	7.123955	-0.039095	3.682243
193.969465	4591.232560	7.128960	-0.039135	3.685313
194.459614	4599.256619	7.133965	-0.039232	3.688397
194.512655	4607.289107	7.138970	-0.039247	3.691470
194.851471	4615.353923	7.143974	-0.039315	3.694560
194.881751	4623.362154	7.148979	-0.039326	3.697618
195.023827	4631.379653	7.153984	-0.039358	3.700679
195.186968	4639.366451	7.158989	-0.039394	3.703727
195.661766	4647.386685	7.163994	-0.039487	3.706793
195.963407	4655.428946	7.168998	-0.039549	3.709861
195.859640	4663.524362	7.174003	-0.039535	3.712936
195.956329	4671.597280	7.179008	-0.039558	3.716005
196.295254	4679.522520	7.184013	-0.039627	3.719021
196.365949	4687.537161	7.189018	-0.039645	3.722062
196.610704	4695.526016	7.194022	-0.039696	3.725095
196.783325	4703.525197	7.199027	-0.039733	3.728128
197.084956	4711.566666	7.204032	-0.039795	3.731177
197.101172	4719.618595	7.209037	-0.039803	3.734221
197.285286	4727.650139	7.214042	-0.039843	3.737259
197.372002	4735.671992	7.219046	-0.039864	3.740288
197.449217	4743.680273	7.224051	-0.039884	3.743309
197.728087	4751.690118	7.229056	-0.039941	3.746334
197.934259	4759.699410	7.234061	-0.039985	3.749354
198.038080	4767.789603	7.239066	-0.040010	3.752399
198.529127	4775.793020	7.244070	-0.040106	3.755418
198.722080	4783.787942	7.249075	-0.040148	3.758425
198.681442	4791.855940	7.254080	-0.040145	3.761452
198.782266	4799.825258	7.259085	-0.040169	3.764442
198.906508	4807.877922	7.264090	-0.040198	3.767461
199.229989	4815.896794	7.269094	-0.040263	3.770470
199.343030	4823.949829	7.274099	-0.040290	3.773485
199.587832	4831.988977	7.279104	-0.040341	3.776495
199.936145	4839.956580	7.284109	-0.040411	3.779478
199.806721	4847.990715	7.289114	-0.040392	3.782473
200.135845	4856.014177	7.294118	-0.040459	3.785472
200.375427	4864.047740	7.299123	-0.040509	3.788470
200.501187	4872.078506	7.304128	-0.040537	3.791462
200.634595	4880.132025	7.309133	-0.040567	3.794460
201.184589	4888.097989	7.314138	-0.040675	3.797433
201.336730	4896.087628	7.319142	-0.040709	3.800403
201.370172	4904.113178	7.324147	-0.040720	3.803382
201.736501	4912.146926	7.329152	-0.040794	3.806368
201.945728	4920.159076	7.334157	-0.040838	3.809341
201.896530	4928.183931	7.339162	-0.040834	3.812311
202.105180	4936.237480	7.344166	-0.040878	3.815294
202.228009	4944.211046	7.349171	-0.040907	3.818244
202.457906	4952.268498	7.354176	-0.040955	3.821224
202.528326	4960.264331	7.359181	-0.040973	3.824176
202.888348	4968.266190	7.364186	-0.041045	3.827134
203.238721	4976.285116	7.369190	-0.041116	3.830096
203.417462	4984.328476	7.374195	-0.041155	3.833061
203.493062	4992.360116	7.379200	-0.041174	3.836018
203.717693	5000.357444	7.384205	-0.041221	3.838962
203.908835	5008.401980	7.389210	-0.041262	3.841921
204.409764	5016.396612	7.394214	-0.041361	3.844865
204.366459	5024.455552	7.399219	-0.041358	3.847820
204.328667	5032.470089	7.404224	-0.041356	3.850756
204.571025	5040.500213	7.409229	-0.041407	3.853701
204.907922	5048.533171	7.414234	-0.041475	3.856647
205.102264	5056.520335	7.419238	-0.041516	3.859571
205.054861	5064.548898	7.424243	-0.041513	3.862503
205.358392	5072.563856	7.429248	-0.041574	3.865435
205.668607	5080.604375	7.434253	-0.041637	3.868374
205.602312	5088.663498	7.439258	-0.041630	3.871311
205.883366	5096.887787	7.444262	-0.041688	3.874311
206.215110	5104.813824	7.449267	-0.041755	3.877202
206.442285	5112.739413	7.454272	-0.041803	3.880089
206.634707	5120.758779	7.459277	-0.041844	3.883007
206.732720	5128.722976	7.464282	-0.041867	3.885901
206.963717	5136.765420	7.469286	-0.041916	3.888823
207.027373	5144.770161	7.474291	-0.041933	3.891727
207.357891	5152.814529	7.479296	-0.042000	3.894647
207.403150	5160.858212	7.484301	-0.042014	3.897560
207.609086	5168.834079	7.489306	-0.042057	3.900449
207.725528	5176.847314	7.494310	-0.042084	3.903348
207.854031	5184.853845	7.499315	-0.042113	3.906242
208.022161	5192.905035	7.504320	-0.042150	3.909151
208.037469	5200.943181	7.509325	-0.042158	3.912051
208.328113	5208.916251	7.514330	-0.042218	3.914930
208.771677	5216.960501	7.519334	-0.042305	3.917835
208.720614	5224.941893	7.524339	-0.042301	3.920706
208.961856	5232.972770	7.529344	-0.042352	3.923598
209.102936	5241.005086	7.534349	-0.042383	3.926487
209.170281	5249.011362	7.539354	-0.042401	3.929363
209.449501	5257.067093	7.544358	-0.042458	3.932258
209.656086	5265.081922	7.549363	-0.042502	3.935135
209.966045	5273.090699	7.554368	-0.042565	3.938010
210.001283	5281.093511	7.559373	-0.042577	3.940876
210.211837	5289.074484	7.564378	-0.042621	3.943735
210.464155	5297.151941	7.569382	-0.042674	3.946627
210.605504	5305.167321	7.574387	-0.042705	3.949492
210.760951	5313.219415	7.579392	-0.042740	3.952369
211.114923	5321.250492	7.584397	-0.042811	3.955240
211.283252	5329.229767	7.589402	-0.042847	3.958087
211.570449	5337.252222	7.594406	-0.042906	3.960949
211.780016	5345.230732	7.599411	-0.042951	3.963792
212.176730	5353.280949	7.604416	-0.043030	3.966662
212.332000	5361.300971	7.609421	-0.043064	3.969515
212.145072	5369.319852	7.614426	-0.043034	3.972360
212.634172	5377.381814	7.619430	-0.043131	3.975229
212.892245	5385.364452	7.624435	-0.043184	3.978064
213.213279	5393.367644	7.629440	-0.043249	3.980905
213.387193	5401.375472	7.634445	-0.043287	3.983744
213.540203	5409.360034	7.639450	-0.043321	3.986572
213.886211	5417.406084	7.644454	-0.043391	3.989422
213.995293	5425.441313	7.649459	-0.043416	3.992263
214.080223	5433.565659	7.654464	-0.043437	3.995134
214.173465	5441.598158	7.659469	-0.043460	3.997969
214.332525	5449.545792	7.664474	-0.043495	4.000774
214.628047	5457.555087	7.669478	-0.043555	4.003601
214.857615	5465.567758	7.674483	-0.043603	4.006425
214.891431	5473.587671	7.679488	-0.043615	4.009248
214.994625	5481.635988	7.684493	-0.043639	4.012079
215.144084	5489.647142	7.689498	-0.043673	4.014896
215.328083	5497.707865	7.694502	-0.043712	4.017729
215.620073	5505.678026	7.699507	-0.043772	4.020530
215.733879	5513.681111	7.704512	-0.043798	4.023337
215.932049	5521.742400	7.709517	-0.043841	4.026165
215.998710	5529.741886	7.714522	-0.043858	4.028966
216.224439	5537.788455	7.719526	-0.043906	4.031785
216.477797	5545.868180	7.724531	-0.043958	4.034613
216.709703	5553.864303	7.729536	-0.044007	4.037410
216.906885	5561.833530	7.734541	-0.044049	4.040196
217.070774	5569.808832	7.739546	-0.044084	4.042980
217.254084	5577.864154	7.744550	-0.044124	4.045791
217.348485	5585.827523	7.749555	-0.044147	4.048567
217.635262	5593.880032	7.754560	-0.044205	4.051375
217.837095	5601.920170	7.759565	-0.044248	4.054175
217.765291	5609.936621	7.764570	-0.044240	4.056961
218.199897	5617.939043	7.769574	-0.044326	4.059747
218.260399	5625.924382	7.774579	-0.044343	4.062521
218.463455	5633.951825	7.779584	-0.044386	4.065309
218.628438	5641.996293	7.784589	-0.044422	4.068100
218.966141	5649.982748	7.789594	-0.044490	4.070872
219.346669	5658.038959	7.794598	-0.044567	4.073666
219.169910	5666.086572	7.799603	-0.044539	4.076448
219.386958	5674.061054	7.804608	-0.044585	4.079208
219.767415	5682.092553	7.809613	-0.044661	4.081989
219.722565	5690.042976	7.814618	-0.044658	4.084733
220.343778	5698.128870	7.819622	-0.044779	4.087531
220.263606	5706.103320	7.824627	-0.044769	4.090280
220.477117	5714.175286	7.829632	-0.044814	4.093064
220.589706	5722.174121	7.834637	-0.044840	4.095820
220.748671	5730.186639	7.839642	-0.044875	4.098579
221.027680	5738.212860	7.844646	-0.044933	4.101343
221.243350	5746.206985	7.849651	-0.044978	4.104093
221.432280	5754.228475	7.854656	-0.045019	4.106850
221.763819	5762.269307	7.859661	-0.045086	4.109613
221.847159	5770.286530	7.864666	-0.045106	4.112364
222.003541	5778.355715	7.869670	-0.045141	4.115131
222.423633	5786.380738	7.874675	-0.045224	4.117885
222.644217	5794.362832	7.879680	-0.045271	4.120619
222.881377	5802.369823	7.884685	-0.045320	4.123361
223.031216	5810.369824	7.889690	-0.045353	4.126097
223.327236	5818.423978	7.894694	-0.045414	4.128851
223.182987	5826.457051	7.899699	-0.045392	4.131592
223.433920	5834.503544	7.904704	-0.045444	4.134339
223.734524	5842.542780	7.909709	-0.045506	4.137083
223.790339	5850.482275	7.914714	-0.045521	4.139788
224.204927	5858.567853	7.919718	-0.045604	4.142546
224.518505	5866.508227	7.924723	-0.045668	4.145251
224.648866	5874.556614	7.929728	-0.045697	4.147988
224.776489	5882.586573	7.934733	-0.045726	4.150718
225.009290	5890.641337	7.939738	-0.045775	4.153455
225.161019	5898.670173	7.944742	-0.045808	4.156181
225.276996	5906.636459	7.949747	-0.045835	4.158884
225.315288	5914.672300	7.954752	-0.045848	4.161607
225.700466	5922.672522	7.959757	-0.045925	4.164320
226.019445	5930.641529	7.964762	-0.045989	4.167020
226.276767	5938.688954	7.969766	-0.046043	4.169745
226.271578	5946.729893	7.974771	-0.046047	4.172462
226.543320	5954.729289	7.979776	-0.046103	4.175167
226.733330	5962.779161	7.984781	-0.046144	4.177886
226.803051	5970.742801	7.989786	-0.046162	4.180572
227.298018	5978.775121	7.994790	-0.046259	4.183285
227.275227	5986.800316	7.999795	-0.046260	4.185988
227.540142	5994.818974	8.004800	-0.046315	4.188690
227.568004	6002.878096	8.009805	-0.046326	4.191402
227.874665	6010.975705	8.014810	-0.046388	4.194127
228.068800	6018.962235	8.019814	-0.046429	4.196812
228.042751	6026.907617	8.024819	-0.046430	4.199480
228.299763	6034.946327	8.029824	-0.046483	4.202180
228.388858	6042.876129	8.034829	-0.046505	4.204840
228.640983	6050.911462	8.039834	-0.046557	4.207535
228.825876	6058.940987	8.044838	-0.046597	4.210226
228.780167	6067.009553	8.049843	-0.046594	4.212926
229.179243	6075.005907	8.054848	-0.046673	4.215604
229.571332	6083.007720	8.059853	-0.046752	4.218282
229.499753	6091.012209	8.064858	-0.046744	4.220955
229.542317	6099.032528	8.069862	-0.046757	4.223633
229.756326	6107.074637	8.074867	-0.046802	4.226318
230.016174	6115.058841	8.079872	-0.046856	4.228982
230.321895	6123.118151	8.084877	-0.046918	4.231671
230.477225	6131.121235	8.089882	-0.046952	4.234337
230.726309	6139.186918	8.094886	-0.047004	4.237023
230.797637	6147.103039	8.099891	-0.047022	4.239656
230.920551	6155.160854	8.104896	-0.047051	4.242335
231.125280	6163.189646	8.109901	-0.047094	4.245003
231.281021	6171.194783	8.114906	-0.047128	4.247662
231.628061	6179.178270	8.119910	-0.047198	4.250313
231.775404	6187.239988	8.124915	-0.047231	4.252987
231.947573	6195.267547	8.129920	-0.047268	4.255647
232.136764	6203.289389	8.134925	-0.047309	4.258305
232.416006	6211.279084	8.139930	-0.047366	4.260951
232.627088	6219.319056	8.144934	-0.047411	4.263611
232.656131	6227.317729	8.149939	-0.047422	4.266254
232.700368	6235.361663	8.154944	-0.047435	4.268911
233.029568	6243.404461	8.159949	-0.047502	4.271568
233.277166	6251.423186	8.164954	-0.047553	4.274215
233.499368	6259.504462	8.169958	-0.047600	4.276881
233.723296	6267.414501	8.174963	-0.047647	4.279488
234.088028	6275.485424	8.179968	-0.047720	4.282148
234.113053	6283.471905	8.184973	-0.047730	4.284776
234.288315	6291.506272	8.189978	-0.047768	4.287419
234.552586	6299.529318	8.194982	-0.047822	4.290058
234.835783	6307.541760	8.199987	-0.047881	4.292691
235.156946	6315.583105	8.204992	-0.047946	4.295333
235.229547	6323.614312	8.209997	-0.047964	4.297967
235.396872	6331.551142	8.215002	-0.048001	4.300570
235.712539	6339.605806	8.220006	-0.048065	4.303211
235.860802	6347.584409	8.225011	-0.048098	4.305824
236.187998	6355.638402	8.230016	-0.048164	4.308461
236.031853	6363.687108	8.235021	-0.048140	4.311092
236.214980	6371.682614	8.240026	-0.048180	4.313706
236.476908	6379.738723	8.245030	-0.048234	4.316339
236.499751	6387.690169	8.250035	-0.048243	4.318934
236.563219	6395.725976	8.255040	-0.048261	4.321556
236.929716	6403.726786	8.260045	-0.048334	4.324166
237.250364	6411.727791	8.265050	-0.048399	4.326775
237.507762	6419.760969	8.270054	-0.048452	4.329392
237.630639	6427.784595	8.275059	-0.048481	4.332004
237.711589	6435.840862	8.280064	-0.048501	4.334624
237.878990	6443.853222	8.285069	-0.048537	4.337229
237.958248	6451.786650	8.290074	-0.048557	4.339806
238.117901	6459.849287	8.295078	-0.048592	4.342424
238.458476	6467.875794	8.300083	-0.048661	4.345030
238.545840	6475.873616	8.305088	-0.048683	4.347624
238.551399	6483.912518	8.310093	-0.048689	4.350229
238.922863	6491.968624	8.315098	-0.048764	4.352839
239.001337	6500.066083	8.320102	-0.048784	4.355460
239.087964	6507.997397	8.325107	-0.048805	4.358026
239.122039	6515.913133	8.330112	-0.048817	4.360585
239.380694	6524.006388	8.335117	-0.048870	4.363201
239.569485	6531.940450	8.340122	-0.048910	4.365763
239.744671	6539.996614	8.345126	-0.048948	4.368364
239.952697	6548.003815	8.350131	-0.048992	4.370947
239.779489	6556.069932	8.355136	-0.048966	4.373545
240.116016	6564.100057	8.360141	-0.049034	4.376133
240.527825	6572.059098	8.365146	-0.049115	4.378697
240.709023	6580.119061	8.370150	-0.049155	4.381291
240.847749	6588.090361	8.375155	-0.049186	4.383855
241.147136	6596.118194	8.380160	-0.049247	4.386436
241.267499	6604.148910	8.385165	-0.049274	4.389015
241.188642	6612.159364	8.390170	-0.049265	4.391585
241.303476	6620.250304	8.395174	-0.049292	4.394181
241.636927	6628.246232	8.400179	-0.049359	4.396746
241.733895	6636.164816	8.405184	-0.049382	4.399283
241.771999	6644.246925	8.410189	-0.049395	4.401871
242.023104	6652.229124	8.415194	-0.049447	4.404426
242.200916	6660.283555	8.420198	-0.049485	4.407003
242.259900	6668.268295	8.425203	-0.049502	4.409555
242.376459	6676.315526	8.430208	-0.049529	4.412126
242.648229	6684.374109	8.435213	-0.049585	4.414700
242.836110	6692.403447	8.440218	-0.049625	4.417262
243.096306	6700.348387	8.445222	-0.049679	4.419797
243.153433	6708.414436	8.450227	-0.049695	4.422367
243.436578	6716.359613	8.455232	-0.049753	4.424899
243.594058	6724.444552	8.460237	-0.049787	4.427473
243.732323	6732.412786	8.465242	-0.049818	4.430009
243.861138	6740.543914	8.470246	-0.049848	4.432594
243.815539	6748.543468	8.475251	-0.049844	4.435136
244.150647	6756.530091	8.480256	-0.049912	4.437673
244.389779	6764.467496	8.485261	-0.049962	4.440193
244.543873	6772.531634	8.490266	-0.049996	4.442752
244.884005	6780.512587	8.495270	-0.050065	4.445283
245.155540	6788.593655	8.500275	-0.050120	4.447845
245.373625	6796.563730	8.505280	-0.050166	4.450369
245.477580	6804.626548	8.510285	-0.050191	4.452921
245.763033	6812.616008	8.515290	-0.050250	4.455449
246.055438	6820.677234	8.520294	-0.050309	4.457998
246.139050	6828.631739	8.525299	-0.050330	4.460511
246.450377	6836.638837	8.530304	-0.050393	4.463040
246.703900	6844.641304	8.535309	-0.050446	4.465566
246.768660	6852.689917	8.540314	-0.050463	4.468105
247.111667	6860.717611	8.545318	-0.050532	4.470636
247.079014	6868.768498	8.550323	-0.050532	4.473172
247.222749	6876.760780	8.555328	-0.050564	4.475689
247.326009	6884.782813	8.560333	-0.050588	4.478213
247.311765	6892.716148	8.565338	-0.050591	4.480708
247.746142	6900.754254	8.570343	-0.050677	4.483236
247.743891	6908.764080	8.575347	-0.050682	4.485752
248.038822	6916.784844	8.580352	-0.050742	4.488270
248.433452	6924.839272	8.585357	-0.050821	4.490799
248.736554	6932.853335	8.590362	-0.050883	4.493312
249.106865	6940.879455	8.595367	-0.050957	4.495829
249.213259	6948.889325	8.600371	-0.050982	4.498338
249.500277	6956.880418	8.605376	-0.051041	4.500840
249.703403	6964.910628	8.610381	-0.051084	4.503353
250.030762	6972.895594	8.615386	-0.051150	4.505851
250.522370	6980.936956	8.620391	-0.051247	4.508365
250.507860	6988.946409	8.625395	-0.051250	4.510867
250.720447	6997.027859	8.630400	-0.051295	4.513390
250.887142	7005.077179	8.635405	-0.051331	4.515901
251.092194	7012.998622	8.640410	-0.051374	4.518372
250.892350	7021.010054	8.645415	-0.051343	4.520868
251.153509	7029.009169	8.650419	-0.051396	4.523360
251.497399	7036.994292	8.655424	-0.051466	4.525847
251.393913	7045.035518	8.660429	-0.051452	4.528348
251.447231	7053.037167	8.665434	-0.051467	4.530836
251.764408	7061.124339	8.670439	-0.051531	4.533350
251.960538	7069.132253	8.675443	-0.051573	4.535838
252.131188	7077.114586	8.680448	-0.051610	4.538316
252.297524	7085.161767	8.685453	-0.051647	4.540813
252.507689	7093.141767	8.690458	-0.051691	4.543288
252.847098	7101.172049	8.695463	-0.051760	4.545777
253.022559	7109.157081	8.700467	-0.051798	4.548251
253.161566	7117.167850	8.705472	-0.051829	4.550731
253.266407	7125.224548	8.710477	-0.051854	4.553224
253.274642	7133.262790	8.715482	-0.051860	4.555709
253.495683	7141.271458	8.720487	-0.051907	4.558185
253.535830	7149.279011	8.725491	-0.051920	4.560658
253.693568	7157.282540	8.730496	-0.051954	4.563129
253.911715	7165.302478	8.735501	-0.052000	4.565604
254.072982	7173.315847	8.740506	-0.052036	4.568076
254.111250	7181.351096	8.745511	-0.052048	4.570552
254.295157	7189.385396	8.750515	-0.052088	4.573027
254.527808	7197.378409	8.755520	-0.052136	4.575489
254.711837	7205.415472	8.760525	-0.052176	4.577962
254.743517	7213.356622	8.765530	-0.052187	4.580404
255.253675	7221.420412	8.770535	-0.052287	4.582883
255.310684	7229.385463	8.775539	-0.052303	4.585330
255.398073	7237.480892	8.780544	-0.052325	4.587816
255.530461	7245.489153	8.785549	-0.052355	4.590273
255.709528	7253.529245	8.790554	-0.052393	4.592740
256.016788	7261.560491	8.795559	-0.052456	4.595202
256.128328	7269.597158	8.800563	-0.052482	4.597664
256.340211	7277.512788	8.805568	-0.052527	4.600088
256.505291	7285.619379	8.810573	-0.052563	4.602569
256.377540	7293.497431	8.815578	-0.052544	4.604979
256.797568	7301.623192	8.820583	-0.052628	4.607463
256.971911	7309.568248	8.825587	-0.052666	4.609891
257.184873	7317.624987	8.830592	-0.052711	4.612351
257.411214	7325.684094	8.835597	-0.052758	4.614811
257.552753	7333.690126	8.840602	-0.052790	4.617253
257.813519	7341.644362	8.845607	-0.052843	4.619678
257.706751	7349.702524	8.850611	-0.052829	4.622134
258.030664	7357.683923	8.855616	-0.052895	4.624565
258.451964	7365.723244	8.860621	-0.052978	4.627012
258.416504	7373.700060	8.865626	-0.052977	4.629439
258.775588	7381.812630	8.870631	-0.053049	4.631906
258.818669	7389.812582	8.875635	-0.053063	4.634337
258.732970	7397.801940	8.880640	-0.053052	4.636764
259.184978	7405.795292	8.885645	-0.053141	4.639191
259.286449	7413.796857	8.890650	-0.053166	4.641619
259.222086	7421.790686	8.895655	-0.053159	4.644043
259.398651	7429.819539	8.900659	-0.053197	4.646477
259.668566	7437.794328	8.905664	-0.053253	4.648892
260.052686	7445.864644	8.910669	-0.053329	4.651336
259.887319	7453.898605	8.915674	-0.053304	4.653767
260.092946	7461.947818	8.920679	-0.053348	4.656202
260.311091	7469.915664	8.925683	-0.053393	4.658611
260.428531	7477.905797	8.930688	-0.053421	4.661025
260.508417	7485.944381	8.935693	-0.053441	4.663453
260.622197	7493.917039	8.940698	-0.053467	4.665859
261.043169	7501.952596	8.945703	-0.053551	4.668283
260.993182	7509.940970	8.950707	-0.053547	4.670692
261.197174	7518.097724	8.955712	-0.053590	4.673149
261.675106	7526.132081	8.960717	-0.053685	4.675569
261.619909	7534.059369	8.965722	-0.053680	4.677956
261.692935	7542.051762	8.970727	-0.053698	4.680360
261.929816	7550.048418	8.975731	-0.053748	4.682765
262.000724	7558.002373	8.980736	-0.053766	4.685156
262.121558	7566.085524	8.985741	-0.053794	4.687584
262.328451	7574.049828	8.990746	-0.053838	4.689975
262.402026	7582.147297	8.995751	-0.053857	4.692405
262.595108	7590.105262	9.000755	-0.053898	4.694792
262.840140	7598.176107	9.005760	-0.053949	4.697211
263.152580	7606.149660	9.010765	-0.054013	4.699600
263.054631	7614.158267	9.015770	-0.054000	4.701999
263.235951	7622.160878	9.020775	-0.054039	4.704394
263.485969	7630.206883	9.025779	-0.054091	4.706801
263.697346	7638.222295	9.030784	-0.054135	4.709197
263.738060	7646.307140	9.035789	-0.054148	4.711614
263.797164	7654.242676	9.040794	-0.054165	4.713984
264.099278	7662.299661	9.045799	-0.054226	4.716389
264.173179	7670.266521	9.050803	-0.054245	4.718767
264.363864	7678.280502	9.055808	-0.054286	4.721157
264.475695	7686.331325	9.060813	-0.054312	4.723556
264.324668	7694.317488	9.065818	-0.054289	4.725937
264.580095	7702.374920	9.070823	-0.054342	4.728336
264.923376	7710.369328	9.075827	-0.054411	4.730714
264.992091	7718.433055	9.080832	-0.054430	4.733113
265.084153	7726.443416	9.085837	-0.054452	4.735495
265.467205	7734.482235	9.090842	-0.054529	4.737883
265.619143	7742.436348	9.095847	-0.054562	4.740245
265.633211	7750.484346	9.100851	-0.054570	4.742635
265.814345	7758.435328	9.105856	-0.054609	4.744994
266.338305	7766.477749	9.110861	-0.054712	4.747378
266.398980	7774.465942	9.115866	-0.054729	4.749746
266.551366	7782.561546	9.120871	-0.054762	4.752144
266.538725	7790.561112	9.125875	-0.054765	4.754513
266.678298	7798.589881	9.130880	-0.054797	4.756889
267.068803	7806.557469	9.135885	-0.054875	4.759245
267.187275	7814.522313	9.140890	-0.054902	4.761600
267.371261	7822.534314	9.145895	-0.054941	4.763968
267.426768	7830.599327	9.150899	-0.054957	4.766350
267.731819	7838.632801	9.155904	-0.055019	4.768721
268.115361	7846.651419	9.160909	-0.055096	4.771086
268.130935	7854.650831	9.165914	-0.055104	4.773445
268.443817	7862.677656	9.170919	-0.055168	4.775811
268.538876	7870.707460	9.175923	-0.055191	4.778176
268.647979	7878.676827	9.180928	-0.055216	4.780523
268.775318	7886.727874	9.185933	-0.055245	4.782893
268.833837	7894.688511	9.190938	-0.055262	4.785235
269.117617	7902.713953	9.195943	-0.055320	4.787594
269.383625	7910.734689	9.200947	-0.055375	4.789950
269.337888	7918.743840	9.205952	-0.055371	4.792304
269.700716	7926.879484	9.210957	-0.055444	4.794691
269.809847	7934.803428	9.215962	-0.055470	4.797017
269.899250	7942.787352	9.220967	-0.055492	4.799358
269.940880	7950.835114	9.225971	-0.055505	4.801718
270.151592	7958.831145	9.230976	-0.055549	4.804060
270.243801	7966.821658	9.235981	-0.055572	4.806401
270.329459	7974.835193	9.240986	-0.055593	4.808747
270.525736	7982.890916	9.245991	-0.055635	4.811103
270.893625	7990.351619	9.250995	-0.055708	4.813283
271.083946	7994.861865	9.256000	-0.055747	4.814601

271.298588	7997.460860	9.261005	-0.055789	4.815360
271.441003	7998.697071	9.266010	-0.055816	4.815720
271.468984	7999.199610	9.271015	-0.055822	4.815867
271.510522	8000.215150	9.276019	-0.055830	4.816164
271.591511	8000.176031	9.281024	-0.055845	4.816152
271.486175	8000.205112	9.286029	-0.055826	4.816161
271.503657	8000.181935	9.291034	-0.055829	4.816154
271.926936	8000.207762	9.296039	-0.055908	4.816159
271.885853	8000.202754	9.301043	-0.055900	4.816158
271.879196	8000.212255	9.306048	-0.055899	4.816161
271.925221	8000.222710	9.311053	-0.055908	4.816164
272.042179	8000.176764	9.316058	-0.055930	4.816150
272.205104	8000.208563	9.321063	-0.055960	4.816158
272.230276	8000.196208	9.326067	-0.055965	4.816154
272.225371	8000.169421	9.331072	-0.055964	4.816147
272.392286	8000.251500	9.336077	-0.055995	4.816170
272.416010	8000.218822	9.341082	-0.056000	4.816160
272.614671	8000.242722	9.346087	-0.056037	4.816166
272.706536	8000.225165	9.351091	-0.056054	4.816160
272.535346	8000.192163	9.356096	-0.056022	4.816152
272.533344	8000.218841	9.361101	-0.056022	4.816159
272.496831	8000.188277	9.366106	-0.056015	4.816151
272.523919	8000.242188	9.371111	-0.056020	4.816166
272.494086	8000.226700	9.376115	-0.056015	4.816162
272.668119	8000.221312	9.381120	-0.056047	4.816159
272.683590	8000.240829	9.386125	-0.056050	4.816165
272.483890	8000.224403	9.391130	-0.056013	4.816161
272.674573	8000.244955	9.396135	-0.056049	4.816166
272.756420	8000.207987	9.401139	-0.056064	4.816155
272.726890	8000.233099	9.406144	-0.056059	4.816163
272.854506	8000.218325	9.411149	-0.056083	4.816158
272.798165	8000.193811	9.416154	-0.056072	4.816151
272.901021	8000.224524	9.421159	-0.056091	4.816159
272.899851	8000.223443	9.426163	-0.056091	4.816159
273.035681	8000.137244	9.431168	-0.056117	4.816133
273.191219	8000.176389	9.436173	-0.056146	4.816143
272.994307	8000.179241	9.441178	-0.056109	4.816145
273.148858	8000.231187	9.446183	-0.056138	4.816160
273.013152	8000.202032	9.451187	-0.056113	4.816152
273.101511	8000.205776	9.456192	-0.056129	4.816153
273.077399	8000.232054	9.461197	-0.056125	4.816160
273.055504	8000.224188	9.466202	-0.056121	4.816158
273.010270	8000.237264	9.471207	-0.056113	4.816162
273.171414	8000.224166	9.476211	-0.056143	4.816158
273.187384	8000.221258	9.481216	-0.056146	4.816157
273.157072	8000.245287	9.486221	-0.056140	4.816164
273.060583	8000.224320	9.491226	-0.056122	4.816158
273.231588	8000.238106	9.496231	-0.056154	4.816161
273.545421	8000.230978	9.501235	-0.056213	4.816158
273.344344	8000.226277	9.506240	-0.056175	4.816157
273.444207	8000.229161	9.511245	-0.056194	4.816158
273.483839	8000.217067	9.516250	-0.056201	4.816154
273.405097	8000.267995	9.521255	-0.056187	4.816169
273.218787	8000.243264	9.526259	-0.056152	4.816163
273.315629	8000.218319	9.531264	-0.056170	4.816155
273.407427	8000.264856	9.536269	-0.056188	4.816168
273.324373	8000.245200	9.541274	-0.056172	4.816163
273.288889	8000.272340	9.546279	-0.056166	4.816171
273.291154	8000.277731	9.551283	-0.056166	4.816173
273.473087	8000.223346	9.556288	-0.056200	4.816156
273.453523	8000.267867	9.561293	-0.056197	4.816169
273.292043	8000.222220	9.566298	-0.056167	4.816156
273.374332	8000.238674	9.571303	-0.056182	4.816161
273.230955	8000.230745	9.576307	-0.056155	4.816159
273.510594	8000.210178	9.581312	-0.056208	4.816152
273.526451	8000.261750	9.586317	-0.056211	4.816167
273.529962	8000.180633	9.591322	-0.056211	4.816143
273.727961	8000.206660	9.596327	-0.056248	4.816149
273.765667	8000.236194	9.601331	-0.056255	4.816158
273.514879	8000.212432	9.606336	-0.056209	4.816152
273.547379	8000.277125	9.611341	-0.056215	4.816171
273.728422	8000.260114	9.616346	-0.056249	4.816165
273.713479	8000.279080	9.621351	-0.056246	4.816171
273.653190	8000.267314	9.626355	-0.056235	4.816168
273.615412	8000.231384	9.631360	-0.056228	4.816157
273.621206	8000.224019	9.636365	-0.056229	4.816155
273.749881	8000.228494	9.641370	-0.056253	4.816156
273.868500	8000.224241	9.646375	-0.056275	4.816154
273.734689	8000.230371	9.651379	-0.056250	4.816156
273.691589	8000.247760	9.656384	-0.056242	4.816162
273.604051	8000.244046	9.661389	-0.056226	4.816161
273.847966	8000.250608	9.666394	-0.056272	4.816162
273.935059	8000.256466	9.671399	-0.056288	4.816163
273.840827	8000.226992	9.676403	-0.056271	4.816155
273.768401	8000.217142	9.681408	-0.056257	4.816152
273.959077	8000.217399	9.686413	-0.056293	4.816151
273.794035	8000.164208	9.691418	-0.056262	4.816137
273.810016	8000.202964	9.696423	-0.056265	4.816148
274.107442	8000.242544	9.701427	-0.056321	4.816158
273.945769	8000.222531	9.706432	-0.056291	4.816153
273.965866	8000.275249	9.711437	-0.056294	4.816168
273.974605	8000.242298	9.716442	-0.056296	4.816158
273.984838	8000.216853	9.721447	-0.056298	4.816151
273.882455	8000.255601	9.726451	-0.056279	4.816163
273.912342	8000.243331	9.731456	-0.056285	4.816159
274.030868	8000.280739	9.736461	-0.056307	4.816169
274.049704	8000.214855	9.741466	-0.056311	4.816150
273.938871	8000.257723	9.746471	-0.056290	4.816163
274.043711	8000.260698	9.751475	-0.056310	4.816163
274.101131	8000.278839	9.756480	-0.056320	4.816168
274.238122	8000.280260	9.761485	-0.056346	4.816168
274.190276	8000.253762	9.766490	-0.056337	4.816161
274.230725	8000.292962	9.771495	-0.056345	4.816172
274.263273	8000.239076	9.776499	-0.056351	4.816156
274.136782	8000.272047	9.781504	-0.056327	4.816166
274.350020	8000.300488	9.786509	-0.056367	4.816173
274.135680	8000.260291	9.791514	-0.056327	4.816163
274.001692	8000.264282	9.796519	-0.056303	4.816165
274.130236	8000.261277	9.801523	-0.056327	4.816163
274.294767	8000.261061	9.806528	-0.056357	4.816162
274.364833	8000.281567	9.811533	-0.056370	4.816168
274.203515	8000.257287	9.816538	-0.056340	4.816162
274.154472	8000.266021	9.821543	-0.056331	4.816164
274.198666	8000.267898	9.826547	-0.056340	4.816165
274.122304	8000.282547	9.831552	-0.056326	4.816169
274.220778	8000.292885	9.836557	-0.056344	4.816172
274.430423	8000.247549	9.841562	-0.056383	4.816158
274.564083	8000.242500	9.846567	-0.056408	4.816155
274.463343	8000.246025	9.851571	-0.056389	4.816157
274.485136	8000.226130	9.856576	-0.056394	4.816151
274.518691	8000.288707	9.861581	-0.056400	4.816169
274.509736	8000.288553	9.866586	-0.056398	4.816169
274.505081	8000.190193	9.871591	-0.056397	4.816140
274.250574	8000.263577	9.876595	-0.056350	4.816163
274.245650	8000.234651	9.881600	-0.056349	4.816155
274.419178	8000.283740	9.886605	-0.056382	4.816168
274.517551	8000.248139	9.891610	-0.056400	4.816157
274.218655	8000.249143	9.896615	-0.056345	4.816159
274.408683	8000.269686	9.901619	-0.056380	4.816164
274.655385	8000.220748	9.906624	-0.056426	4.816148
274.443541	8000.238284	9.911629	-0.056387	4.816155
274.303746	8000.240033	9.916634	-0.056361	4.816156
274.340250	8000.246044	9.921639	-0.056368	4.816158
274.392494	8000.260886	9.926643	-0.056377	4.816162
274.287476	8000.244035	9.931648	-0.056358	4.816157
274.391085	8000.276901	9.936653	-0.056377	4.816166
274.480855	8000.266784	9.941658	-0.056394	4.816163
274.361271	8000.272103	9.946663	-0.056372	4.816165
274.301327	8000.274230	9.951667	-0.056361	4.816166
274.418636	8000.247519	9.956672	-0.056383	4.816158
274.520329	8000.281419	9.961677	-0.056402	4.816167
274.389541	8000.239530	9.966682	-0.056378	4.816155
274.480568	8000.236914	9.971687	-0.056395	4.816154
274.474974	8000.249640	9.976691	-0.056394	4.816158
274.362868	8000.207022	9.981696	-0.056373	4.816146
274.539539	8000.271124	9.986701	-0.056406	4.816164
274.439300	8000.258633	9.991706	-0.056387	4.816161
274.394404	8000.272783	9.996711	-0.056379	4.816165
274.678657	8000.281146	10.001715	-0.056432	4.816166
274.755983	8000.240891	10.006720	-0.056446	4.816154
274.581290	8000.287944	10.011725	-0.056414	4.816168
274.547995	8000.221114	10.016730	-0.056408	4.816149
274.726840	8000.225431	10.021735	-0.056441	4.816149
274.776952	8000.265874	10.026739	-0.056451	4.816161
274.642612	8000.250628	10.031744	-0.056426	4.816157
274.589011	8000.281714	10.036749	-0.056416	4.816167
274.524523	8000.264529	10.041754	-0.056404	4.816162
274.654575	8000.234844	10.046759	-0.056428	4.816153
274.528204	8000.256066	10.051763	-0.056405	4.816159
274.346553	8000.217529	10.056768	-0.056371	4.816149
274.550536	8000.262896	10.061773	-0.056409	4.816161
274.551226	8000.231936	10.066778	-0.056409	4.816152
274.568906	8000.279269	10.071783	-0.056413	4.816166
274.706413	8000.267881	10.076787	-0.056438	4.816162
274.570820	8000.244066	10.081792	-0.056413	4.816156
274.688653	8000.284668	10.086797	-0.056435	4.816167
274.554119	8000.257667	10.091802	-0.056410	4.816160
274.740502	8000.219388	10.096807	-0.056445	4.816148
274.708348	8000.252999	10.101811	-0.056439	4.816158
274.638565	8000.229309	10.106816	-0.056426	4.816151
274.602138	8000.278867	10.111821	-0.056420	4.816166
274.527800	8000.283938	10.116826	-0.056406	4.816168
274.567698	8000.255825	10.121831	-0.056413	4.816159
274.754189	8000.261348	10.126835	-0.056448	4.816160
274.612646	8000.231016	10.131840	-0.056422	4.816152
274.604372	8000.260786	10.136845	-0.056420	4.816160
274.635667	8000.235722	10.141850	-0.056426	4.816153
274.837457	8000.226566	10.146855	-0.056464	4.816149
274.763235	8000.258347	10.151859	-0.056450	4.816159
274.873876	8000.250745	10.156864	-0.056471	4.816156
274.950270	8000.311962	10.161869	-0.056485	4.816173
274.988125	8000.253899	10.166874	-0.056492	4.816156
274.941256	8000.210325	10.171879	-0.056484	4.816144
274.887491	8000.288414	10.176883	-0.056474	4.816167
274.951322	8000.271417	10.181888	-0.056486	4.816162
274.776785	8000.281083	10.186893	-0.056453	4.816165
275.002167	8000.275560	10.191898	-0.056495	4.816163
274.783609	8000.295110	10.196903	-0.056455	4.816169
274.611906	8000.258890	10.201907	-0.056423	4.816160
274.706009	8000.223212	10.206912	-0.056440	4.816149
274.944838	8000.290577	10.211917	-0.056485	4.816167
274.909799	8000.287814	10.216922	-0.056479	4.816167
274.866380	8000.238961	10.221927	-0.056471	4.816153
274.814231	8000.266869	10.226931	-0.056461	4.816161
274.783028	8000.253492	10.231936	-0.056455	4.816157
274.818301	8000.259480	10.236941	-0.056462	4.816159
274.949592	8000.242637	10.241946	-0.056486	4.816153
275.013445	8000.241666	10.246951	-0.056498	4.816153
274.926731	8000.272152	10.251955	-0.056482	4.816162
274.760630	8000.274492	10.256960	-0.056451	4.816163
275.034050	8000.279454	10.261965	-0.056502	4.816163
275.082780	8000.235476	10.266970	-0.056512	4.816150
275.035833	8000.251726	10.271975	-0.056503	4.816155
275.018817	8000.271724	10.276979	-0.056500	4.816161
274.992060	8000.230651	10.281984	-0.056495	4.816149
274.926827	8000.291439	10.286989	-0.056483	4.816168
274.944567	8000.254378	10.291994	-0.056486	4.816157
275.126141	8000.212806	10.296999	-0.056520	4.816143
275.048731	8000.257349	10.302003	-0.056506	4.816157
274.956594	8000.242868	10.307008	-0.056489	4.816153
275.111548	8000.284143	10.312013	-0.056518	4.816164
275.300599	8000.261937	10.317018	-0.056553	4.816157
274.994174	8000.236095	10.322023	-0.056496	4.816151
275.034694	8000.284911	10.327027	-0.056504	4.816165
275.158522	8000.236952	10.332032	-0.056527	4.816150
275.217267	8000.243366	10.337037	-0.056538	4.816152
275.063860	8000.234184	10.342042	-0.056509	4.816150
275.039498	8000.219863	10.347047	-0.056505	4.816146
275.146475	8000.241039	10.352051	-0.056525	4.816152
274.995269	8000.209463	10.357056	-0.056497	4.816143
275.244703	8000.248176	10.362061	-0.056543	4.816153
275.335270	8000.272260	10.367066	-0.056560	4.816160
275.176688	8000.327084	10.372071	-0.056531	4.816177
275.073107	8000.311327	10.377075	-0.056512	4.816173
274.961244	8000.244140	10.382080	-0.056491	4.816153
275.161268	8000.283027	10.387085	-0.056528	4.816164
275.087585	8000.273153	10.392090	-0.056515	4.816161
275.194094	8000.240905	10.397095	-0.056534	4.816151
275.168658	8000.286390	10.402099	-0.056530	4.816165
275.185739	8000.242906	10.407104	-0.056533	4.816152
275.248844	8000.320977	10.412109	-0.056545	4.816174
275.234961	8000.299367	10.417114	-0.056542	4.816168
275.042188	8000.264901	10.422119	-0.056507	4.816159
275.248555	8000.250487	10.427123	-0.056545	4.816154
275.217561	8000.252070	10.432128	-0.056539	4.816154
275.122229	8000.297356	10.437133	-0.056522	4.816168
275.148538	8000.281816	10.442138	-0.056527	4.816163
275.111538	8000.270470	10.447143	-0.056520	4.816160
275.165590	8000.300303	10.452147	-0.056530	4.816169
275.063001	8000.270675	10.457152	-0.056511	4.816161
275.104999	8000.286401	10.462157	-0.056519	4.816165
275.110950	8000.249125	10.467162	-0.056520	4.816154
275.060646	8000.251427	10.472167	-0.056511	4.816155
275.049267	8000.262980	10.477171	-0.056509	4.816158
275.095325	8000.248866	10.482176	-0.056517	4.816154
274.989169	8000.265112	10.487181	-0.056498	4.816159
275.080705	8000.259300	10.492186	-0.056515	4.816157
275.126584	8000.214202	10.497191	-0.056523	4.816144
275.223419	8000.266176	10.502195	-0.056542	4.816158
275.075199	8000.242131	10.507200	-0.056514	4.816152
275.149460	8000.269125	10.512205	-0.056528	4.816160
275.088610	8000.260552	10.517210	-0.056517	4.816158
275.026925	8000.213505	10.522215	-0.056505	4.816144
275.120796	8000.259014	10.527219	-0.056523	4.816157
275.122705	8000.246237	10.532224	-0.056523	4.816153
275.284980	8000.284440	10.537229	-0.056554	4.816163
275.015993	8000.250729	10.542234	-0.056504	4.816155
275.073410	8000.232548	10.547239	-0.056514	4.816149
275.182149	8000.274054	10.552243	-0.056535	4.816161
275.241478	8000.240951	10.557248	-0.056546	4.816151
275.227479	8000.259935	10.562253	-0.056543	4.816157
275.360065	8000.277302	10.567258	-0.056568	4.816161
275.362943	8000.227151	10.572263	-0.056569	4.816146
275.473004	8000.280433	10.577267	-0.056589	4.816161
275.416817	8000.279423	10.582272	-0.056579	4.816161
275.293510	8000.255830	10.587277	-0.056556	4.816155
275.253819	8000.249777	10.592282	-0.056549	4.816153
275.190877	8000.210185	10.597287	-0.056537	4.816142
275.393314	8000.277961	10.602291	-0.056575	4.816161
275.177275	8000.266576	10.607296	-0.056535	4.816159
275.251570	8000.291433	10.612301	-0.056549	4.816166
275.140276	8000.256306	10.617306	-0.056528	4.816156
275.144135	8000.202968	10.622311	-0.056529	4.816140
275.267522	8000.288541	10.627315	-0.056552	4.816165
275.430481	8000.243428	10.632320	-0.056582	4.816151
275.507991	8000.277958	10.637325	-0.056597	4.816160
275.168288	8000.231214	10.642330	-0.056534	4.816148
275.485377	8000.192098	10.647335	-0.056593	4.816135
275.445492	8000.249073	10.652339	-0.056585	4.816152
275.364624	8000.248684	10.657344	-0.056570	4.816153
275.564689	8000.275821	10.662349	-0.056608	4.816159
275.545992	8000.214595	10.667354	-0.056604	4.816142
275.526249	8000.250569	10.672359	-0.056601	4.816152
275.367367	8000.301114	10.677363	-0.056571	4.816168
275.268030	8000.262998	10.682368	-0.056553	4.816157
275.567795	8000.278054	10.687373	-0.056609	4.816160
275.423490	8000.280788	10.692378	-0.056582	4.816162
275.422859	8000.267965	10.697383	-0.056582	4.816158
275.537709	8000.299967	10.702387	-0.056603	4.816167
275.299904	8000.249728	10.707392	-0.056559	4.816153
275.405433	8000.302928	10.712397	-0.056579	4.816168
275.564755	8000.294072	10.717402	-0.056609	4.816165
275.430625	8000.271350	10.722407	-0.056584	4.816159
275.614927	8000.281109	10.727411	-0.056618	4.816161
275.573679	8000.210928	10.732416	-0.056611	4.816140
275.801654	8000.250322	10.737421	-0.056653	4.816151
275.744135	8000.263176	10.742426	-0.056642	4.816155
275.591589	8000.255078	10.747431	-0.056614	4.816153
275.635522	8000.279385	10.752435	-0.056622	4.816160
275.561715	8000.267372	10.757440	-0.056609	4.816157
275.471880	8000.298870	10.762445	-0.056592	4.816167
275.636430	8000.270879	10.767450	-0.056623	4.816158
275.573008	8000.240893	10.772455	-0.056611	4.816149
275.661446	8000.282032	10.777459	-0.056628	4.816161
275.479993	8000.239223	10.782464	-0.056594	4.816149
275.452447	8000.244073	10.787469	-0.056589	4.816151
275.644971	8000.262527	10.792474	-0.056625	4.816155
275.402735	8000.265623	10.797479	-0.056580	4.816157
275.516321	8000.292261	10.802483	-0.056601	4.816164
275.367150	8000.225466	10.807488	-0.056573	4.816146
275.417613	8000.292625	10.812493	-0.056583	4.816165
275.586687	8000.281809	10.817498	-0.056614	4.816161
275.637364	8000.265642	10.822503	-0.056624	4.816156
275.568273	8000.291106	10.827507	-0.056611	4.816164
275.418620	8000.227507	10.832512	-0.056583	4.816146
275.577459	8000.289152	10.837517	-0.056613	4.816163
275.341686	8000.264589	10.842522	-0.056569	4.816157
275.520976	8000.246479	10.847527	-0.056603	4.816151
275.556766	8000.269571	10.852531	-0.056609	4.816158
275.418882	8000.233962	10.857536	-0.056584	4.816148
275.296593	8000.271282	10.862541	-0.056561	4.816159
275.434078	8000.258825	10.867546	-0.056587	4.816155
275.507504	8000.202474	10.872551	-0.056601	4.816138
275.459644	8000.292422	10.877555	-0.056592	4.816165
275.535993	8000.261764	10.882560	-0.056606	4.816155
275.781038	8000.244847	10.887565	-0.056652	4.816149
275.673666	8000.249318	10.892570	-0.056632	4.816151
275.671463	8000.266380	10.897575	-0.056632	4.816156
275.900651	8000.296182	10.902579	-0.056674	4.816163
275.761783	8000.257350	10.907584	-0.056648	4.816153
275.718125	8000.321735	10.912589	-0.056640	4.816172
275.596989	8000.299249	10.917594	-0.056618	4.816166
275.698786	8000.265847	10.922599	-0.056637	4.816156
275.707092	8000.334379	10.927603	-0.056639	4.816176
275.583051	8000.280858	10.932608	-0.056616	4.816161
275.596319	8000.271492	10.937613	-0.056618	4.816158
275.560681	8000.260171	10.942618	-0.056612	4.816155
275.567927	8000.264583	10.947623	-0.056613	4.816156
275.662741	8000.257763	10.952627	-0.056631	4.816153
275.648061	8000.254300	10.957632	-0.056628	4.816153
275.507996	8000.265658	10.962637	-0.056602	4.816157
275.568986	8000.289206	10.967642	-0.056614	4.816163
275.563650	8000.228222	10.972647	-0.056613	4.816145
275.819357	8000.293760	10.977651	-0.056660	4.816163
275.620218	8000.259177	10.982656	-0.056623	4.816154
275.624628	8000.273153	10.987661	-0.056624	4.816158
275.574409	8000.280798	10.992666	-0.056615	4.816161
275.603129	8000.242866	10.997671	-0.056620	4.816149
275.748690	8000.310681	11.002675	-0.056648	4.816168
275.608520	8000.292123	11.007680	-0.056622	4.816164
275.654275	8000.289755	11.012685	-0.056630	4.816163
275.779496	8000.270666	11.017690	-0.056654	4.816157
275.848110	8000.271918	11.022695	-0.056666	4.816157
275.822667	8000.289627	11.027699	-0.056662	4.816162
275.536005	8000.253457	11.032704	-0.056608	4.816153
275.554134	8000.284775	11.037709	-0.056612	4.816162
275.704470	8000.305670	11.042714	-0.056640	4.816167
275.562256	8000.272119	11.047719	-0.056614	4.816158
275.687919	8000.336368	11.052723	-0.056637	4.816176
275.772483	8000.294107	11.057728	-0.056653	4.816163
275.939555	8000.308895	11.062733	-0.056684	4.816167
275.865887	8000.249877	11.067738	-0.056670	4.816150
275.833475	8000.267459	11.072743	-0.056665	4.816155
275.920071	8000.295745	11.077747	-0.056681	4.816163
275.627657	8000.286180	11.082752	-0.056626	4.816162
275.819616	8000.301419	11.087757	-0.056662	4.816165
275.797357	8000.314912	11.092762	-0.056658	4.816169
275.630878	8000.290536	11.097767	-0.056627	4.816163
275.735636	8000.309536	11.102771	-0.056647	4.816168
275.826086	8000.284475	11.107776	-0.056664	4.816160
275.868926	8000.269234	11.112781	-0.056672	4.816156
275.698738	8000.271499	11.117786	-0.056640	4.816157
275.736324	8000.297828	11.122791	-0.056647	4.816165
275.995433	8000.334584	11.127795	-0.056696	4.816174
275.655943	8000.286772	11.132800	-0.056632	4.816162
275.844448	8000.308359	11.137805	-0.056668	4.816167
276.071402	8000.272952	11.142810	-0.056710	4.816156
275.904155	8000.280612	11.147815	-0.056679	4.816159
275.879135	8000.304738	11.152819	-0.056674	4.816166
275.985831	8000.301339	11.157824	-0.056694	4.816164
276.061147	8000.288824	11.162829	-0.056708	4.816160
275.989762	8000.288606	11.167834	-0.056695	4.816161
275.768360	8000.304899	11.172839	-0.056654	4.816167
275.782807	8000.303032	11.177843	-0.056657	4.816166
275.802099	8000.286296	11.182848	-0.056661	4.816161
275.797494	8000.331091	11.187853	-0.056660	4.816174
275.842845	8000.331921	11.192858	-0.056668	4.816174
275.730058	8000.319201	11.197863	-0.056647	4.816171
275.879990	8000.328337	11.202867	-0.056675	4.816173
275.815591	8000.285513	11.207872	-0.056663	4.816161
275.782203	8000.245387	11.212877	-0.056657	4.816149
275.922082	8000.252204	11.217882	-0.056683	4.816150
275.808682	8000.257634	11.222887	-0.056662	4.816153
276.029910	8000.301181	11.227891	-0.056704	4.816164
275.995690	8000.273860	11.232896	-0.056697	4.816156
275.901376	8000.320234	11.237901	-0.056680	4.816170
275.960510	8000.312767	11.242906	-0.056691	4.816168
275.873399	8000.284488	11.247911	-0.056675	4.816160
275.781764	8000.298860	11.252915	-0.056658	4.816165
275.815892	8000.280256	11.257920	-0.056664	4.816159
275.834601	8000.310517	11.262925	-0.056668	4.816168
275.736073	8000.280962	11.267930	-0.056650	4.816160
275.811815	8000.281275	11.272935	-0.056664	4.816159
275.931647	8000.304822	11.277939	-0.056686	4.816166
275.904426	8000.284038	11.282944	-0.056681	4.816160
275.955683	8000.326640	11.287949	-0.056691	4.816172
276.179677	8000.336051	11.292954	-0.056733	4.816173
276.161961	8000.294072	11.297959	-0.056729	4.816161
276.174574	8000.337043	11.302963	-0.056732	4.816174
276.159257	8000.290834	11.307968	-0.056729	4.816160
276.022956	8000.281961	11.312973	-0.056704	4.816158
275.849940	8000.284174	11.317978	-0.056672	4.816160
275.788670	8000.283072	11.322983	-0.056660	4.816160
276.041869	8000.323993	11.327987	-0.056708	4.816171
275.811587	8000.295255	11.332992	-0.056665	4.816163
275.765507	8000.273061	11.337997	-0.056656	4.816157
276.031053	8000.289634	11.343002	-0.056706	4.816161
275.835795	8000.231617	11.348007	-0.056669	4.816145
275.994533	8000.329585	11.353011	-0.056699	4.816173
275.880002	8000.306150	11.358016	-0.056678	4.816166
275.982772	8000.309089	11.363021	-0.056697	4.816167
276.049174	8000.335941	11.368026	-0.056710	4.816174
275.952359	8000.280777	11.373031	-0.056692	4.816158
276.021112	8000.332244	11.378035	-0.056705	4.816173
275.964266	8000.279940	11.383040	-0.056694	4.816158
276.004422	8000.260378	11.388045	-0.056702	4.816152
276.010112	8000.260489	11.393050	-0.056703	4.816152
275.976712	8000.268438	11.398055	-0.056697	4.816155
276.043409	8000.300637	11.403059	-0.056709	4.816164
276.117599	8000.295580	11.408064	-0.056723	4.816162
276.148654	8000.308971	11.413069	-0.056729	4.816166
276.021497	8000.292786	11.418074	-0.056705	4.816162
276.076529	8000.289518	11.423079	-0.056716	4.816160
276.087840	8000.300414	11.428083	-0.056718	4.816163
276.065629	8000.292541	11.433088	-0.056714	4.816161
275.845335	8000.306718	11.438093	-0.056673	4.816167
276.089208	8000.302600	11.443098	-0.056718	4.816164
276.139046	8000.271461	11.448103	-0.056728	4.816155
276.126821	8000.315049	11.453107	-0.056725	4.816168
275.977123	8000.286703	11.458112	-0.056698	4.816160
276.183086	8000.297924	11.463117	-0.056736	4.816162
276.278633	8000.321031	11.468122	-0.056754	4.816168
276.109624	8000.300881	11.473127	-0.056723	4.816163
276.080435	8000.333479	11.478131	-0.056717	4.816173
276.131961	8000.314122	11.483136	-0.056727	4.816167
275.948690	8000.311876	11.488141	-0.056693	4.816168
276.090284	8000.300562	11.493146	-0.056719	4.816163
276.156409	8000.324205	11.498151	-0.056732	4.816170
276.005169	8000.324676	11.503155	-0.056704	4.816171
275.879639	8000.299973	11.508160	-0.056680	4.816164
276.141139	8000.334635	11.513165	-0.056729	4.816173
276.028707	8000.325127	11.518170	-0.056708	4.816171
275.838090	8000.303517	11.523175	-0.056673	4.816166
276.040411	8000.352063	11.528179	-0.056711	4.816179
275.967975	8000.293067	11.533184	-0.056697	4.816162
275.854166	8000.310243	11.538189	-0.056676	4.816168
275.949003	8000.304491	11.543194	-0.056694	4.816165
276.164407	8000.305199	11.548199	-0.056734	4.816164
276.199733	8000.303711	11.553203	-0.056741	4.816164
275.993944	8000.245503	11.558208	-0.056702	4.816148
276.123498	8000.290593	11.563213	-0.056727	4.816160
276.253169	8000.317524	11.568218	-0.056751	4.816168
276.053555	8000.313913	11.573223	-0.056714	4.816168
276.154814	8000.344602	11.578227	-0.056733	4.816176
275.976389	8000.297573	11.583232	-0.056700	4.816163
276.150560	8000.319969	11.588237	-0.056732	4.816169
276.044846	8000.307377	11.593242	-0.056712	4.816166
275.979075	8000.297646	11.598247	-0.056700	4.816163
275.992211	8000.310712	11.603251	-0.056703	4.816167
275.877149	8000.289404	11.608256	-0.056681	4.816161
276.194927	8000.322950	11.613261	-0.056741	4.816169
276.171032	8000.294748	11.618266	-0.056736	4.816161
275.958481	8000.297313	11.623271	-0.056697	4.816163
275.906961	8000.302797	11.628275	-0.056687	4.816165
276.017998	8000.301612	11.633280	-0.056708	4.816164
276.108104	8000.329963	11.638285	-0.056725	4.816172
276.156400	8000.312684	11.643290	-0.056734	4.816167
276.074765	8000.269547	11.648295	-0.056719	4.816154
276.243701	8000.313215	11.653299	-0.056750	4.816166
275.922800	8000.283902	11.658304	-0.056691	4.816159
276.097267	8000.319123	11.663309	-0.056723	4.816169
276.333075	8000.313791	11.668314	-0.056767	4.816166
276.222526	8000.267992	11.673319	-0.056747	4.816153
276.240558	8000.319608	11.678323	-0.056750	4.816168
276.106203	8000.286198	11.683328	-0.056725	4.816159
276.220856	8000.329950	11.688333	-0.056747	4.816171
276.253322	8000.336957	11.693338	-0.056753	4.816173
276.087651	8000.283749	11.698343	-0.056722	4.816158
276.256875	8000.304987	11.703347	-0.056754	4.816164
275.998749	8000.274675	11.708352	-0.056706	4.816156
276.084870	8000.304021	11.713357	-0.056722	4.816164
276.118267	8000.276857	11.718362	-0.056728	4.816156
276.013628	8000.286720	11.723367	-0.056709	4.816160
275.980509	8000.319247	11.728371	-0.056703	4.816169
276.043976	8000.286218	11.733376	-0.056715	4.816159
276.220700	8000.327890	11.738381	-0.056748	4.816171
276.177364	8000.330318	11.743386	-0.056740	4.816172
276.040768	8000.301141	11.748391	-0.056714	4.816164
276.333322	8000.333161	11.753395	-0.056769	4.816172
276.239756	8000.307969	11.758400	-0.056751	4.816165
275.990743	8000.331240	11.763405	-0.056705	4.816173
276.047830	8000.309847	11.768410	-0.056716	4.816166
276.093967	8000.303213	11.773415	-0.056725	4.816164
276.158187	8000.332163	11.778419	-0.056737	4.816172
276.097741	8000.305434	11.783424	-0.056725	4.816165
276.195395	8000.347810	11.788429	-0.056744	4.816177
276.226391	8000.340902	11.793434	-0.056750	4.816174
276.093657	8000.301111	11.798439	-0.056725	4.816163
276.278288	8000.314081	11.803443	-0.056759	4.816166
276.225918	8000.307798	11.808448	-0.056750	4.816165
276.256034	8000.342540	11.813453	-0.056755	4.816175
276.415243	8000.328341	11.818458	-0.056785	4.816170
276.055231	8000.298318	11.823463	-0.056718	4.816163
276.006513	8000.318809	11.828467	-0.056709	4.816169
275.959753	8000.266689	11.833472	-0.056701	4.816154
276.033385	8000.346021	11.838477	-0.056714	4.816177
275.932918	8000.323909	11.843482	-0.056696	4.816171
275.958734	8000.277378	11.848487	-0.056701	4.816157
276.130922	8000.320036	11.853491	-0.056733	4.816169
276.166217	8000.297181	11.858496	-0.056739	4.816162
276.249254	8000.346770	11.863501	-0.056755	4.816176
276.290110	8000.329357	11.868506	-0.056763	4.816171
276.076788	8000.290242	11.873511	-0.056723	4.816160
276.089565	8000.316122	11.878515	-0.056725	4.816168
276.015553	8000.295558	11.883520	-0.056712	4.816162
276.112134	8000.300521	11.888525	-0.056730	4.816163
276.205866	8000.333211	11.893530	-0.056747	4.816172
276.092080	8000.314062	11.898535	-0.056726	4.816167
276.267707	8000.317255	11.903539	-0.056759	4.816167
276.086004	8000.286191	11.908544	-0.056725	4.816159
276.174505	8000.316649	11.913549	-0.056742	4.816168
276.171856	8000.333703	11.918554	-0.056741	4.816173
276.084252	8000.334259	11.923559	-0.056725	4.816173
276.174100	8000.346580	11.928563	-0.056742	4.816176
276.121557	8000.314653	11.933568	-0.056732	4.816167
276.081324	8000.328888	11.938573	-0.056725	4.816172
276.085341	8000.327901	11.943578	-0.056726	4.816171
276.180259	8000.283690	11.948583	-0.056743	4.816158
276.488835	8000.326686	11.953587	-0.056801	4.816169
276.256336	8000.309658	11.958592	-0.056758	4.816165
276.096582	8000.302496	11.963597	-0.056728	4.816164
276.225415	8000.321933	11.968602	-0.056752	4.816169
276.131564	8000.310625	11.973607	-0.056735	4.816166
276.259753	8000.326845	11.978611	-0.056759	4.816170
276.150210	8000.300295	11.983616	-0.056738	4.816163
276.231649	8000.319942	11.988621	-0.056754	4.816168
276.159463	8000.323983	11.993626	-0.056740	4.816170
276.120862	8000.306197	11.998631	-0.056733	4.816165
276.149664	8000.327026	12.003635	-0.056739	4.816171
276.106421	8000.287789	12.008640	-0.056731	4.816159
276.103735	8000.315526	12.013645	-0.056730	4.816168
276.134139	8000.320358	12.018650	-0.056736	4.816169
276.206069	8000.309919	12.023655	-0.056750	4.816165
276.227970	8000.333827	12.028659	-0.056754	4.816172
276.239857	8000.307342	12.033664	-0.056756	4.816164
276.407202	8000.311453	12.038669	-0.056787	4.816165
276.464158	8000.342407	12.043674	-0.056798	4.816173
276.272137	8000.310088	12.048679	-0.056762	4.816165
276.343259	8000.321001	12.053683	-0.056776	4.816168
276.370837	8000.317235	12.058688	-0.056781	4.816167
276.326083	8000.313227	12.063693	-0.056773	4.816166
276.271359	8000.313311	12.068698	-0.056762	4.816166
276.367995	8000.287294	12.073703	-0.056781	4.816158
276.215771	8000.292020	12.078707	-0.056752	4.816160
276.284759	8000.291142	12.083712	-0.056765	4.816159
276.246146	8000.284040	12.088717	-0.056758	4.816158
276.248913	8000.325764	12.093722	-0.056759	4.816170
276.256409	8000.288516	12.098727	-0.056760	4.816159
276.322898	8000.328190	12.103731	-0.056773	4.816170
276.283023	8000.284741	12.108736	-0.056765	4.816158
276.262598	8000.313224	12.113741	-0.056762	4.816166
276.347263	8000.339339	12.118746	-0.056777	4.816173
276.345599	8000.322223	12.123751	-0.056777	4.816168
276.525750	8000.335113	12.128755	-0.056811	4.816171
276.354354	8000.315988	12.133760	-0.056779	4.816166
276.316194	8000.321714	12.138765	-0.056772	4.816168
276.401203	8000.331810	12.143770	-0.056788	4.816171
276.210870	8000.318752	12.148775	-0.056752	4.816168
276.235099	8000.328815	12.153779	-0.056757	4.816171
276.329161	8000.312366	12.158784	-0.056775	4.816165
276.262506	8000.315439	12.163789	-0.056762	4.816167
276.179542	8000.329968	12.168794	-0.056747	4.816171
276.363601	8000.296989	12.173799	-0.056781	4.816161
276.465671	8000.342651	12.178803	-0.056800	4.816173
276.251331	8000.309927	12.183808	-0.056761	4.816165
276.145198	8000.334719	12.188813	-0.056741	4.816173
276.301398	8000.326876	12.193818	-0.056770	4.816170
276.350720	8000.316026	12.198823	-0.056779	4.816166
276.362255	8000.330132	12.203827	-0.056782	4.816170
276.524772	8000.298899	12.208832	-0.056812	4.816160
276.357740	8000.305494	12.213837	-0.056781	4.816163
276.308300	8000.322767	12.218842	-0.056772	4.816168
276.413600	8000.314001	12.223847	-0.056791	4.816165
276.408291	8000.320323	12.228851	-0.056791	4.816167
276.300114	8000.315164	12.233856	-0.056771	4.816166
276.273593	8000.333922	12.238861	-0.056766	4.816172
276.273059	8000.330715	12.243866	-0.056766	4.816171
276.161477	8000.310538	12.248871	-0.056745	4.816166
276.390317	8000.327515	12.253875	-0.056788	4.816169
276.479708	8000.305640	12.258880	-0.056804	4.816163
276.478695	8000.334476	12.263885	-0.056804	4.816171
276.394724	8000.314799	12.268890	-0.056789	4.816166
276.607726	8000.328284	12.273895	-0.056828	4.816168
276.649721	8000.322644	12.278899	-0.056836	4.816167
276.272935	8000.324367	12.283904	-0.056766	4.816169
276.314873	8000.327272	12.288909	-0.056774	4.816170
276.344554	8000.321408	12.293914	-0.056780	4.816168
276.388846	8000.258117	12.298919	-0.056788	4.816149
276.339830	8000.341637	12.303923	-0.056779	4.816174
276.304371	8000.301473	12.308928	-0.056773	4.816162
276.281836	8000.341670	12.313933	-0.056768	4.816174
276.232568	8000.317281	12.318938	-0.056759	4.816167
276.283544	8000.312871	12.323943	-0.056769	4.816166
276.393301	8000.340510	12.328947	-0.056789	4.816173
276.305210	8000.300460	12.333952	-0.056773	4.816162
276.345794	8000.308682	12.338957	-0.056781	4.816164
276.565068	8000.319076	12.343962	-0.056822	4.816166
276.474387	8000.300346	12.348967	-0.056805	4.816161
276.342481	8000.338560	12.353971	-0.056780	4.816173
276.324192	8000.317937	12.358976	-0.056777	4.816167
276.307850	8000.332606	12.363981	-0.056774	4.816171
276.326941	8000.328687	12.368986	-0.056778	4.816170
276.303866	8000.298362	12.373991	-0.056773	4.816161
276.562215	8000.327627	12.378995	-0.056822	4.816168
276.453260	8000.290404	12.384000	-0.056801	4.816158
276.435092	8000.310381	12.389005	-0.056798	4.816164
276.582254	8000.339766	12.394010	-0.056826	4.816172
276.283538	8000.319401	12.399015	-0.056770	4.816168
276.403527	8000.327995	12.404019	-0.056793	4.816169
276.358747	8000.301550	12.409024	-0.056784	4.816162
276.615483	8000.342538	12.414029	-0.056832	4.816173
276.410573	8000.332420	12.419034	-0.056794	4.816171
276.213182	8000.322439	12.424039	-0.056757	4.816169
276.525889	8000.345210	12.429043	-0.056816	4.816174
276.389360	8000.296803	12.434048	-0.056790	4.816160
276.429464	8000.292197	12.439053	-0.056798	4.816159
276.566309	8000.312848	12.444058	-0.056824	4.816164
276.405058	8000.284292	12.449063	-0.056794	4.816157
276.337902	8000.288424	12.454067	-0.056781	4.816158
276.444123	8000.278606	12.459072	-0.056801	4.816155
276.646699	8000.299381	12.464077	-0.056839	4.816160
276.589251	8000.336808	12.469082	-0.056828	4.816171
276.432472	8000.280555	12.474087	-0.056799	4.816155
276.714619	8000.314525	12.479091	-0.056852	4.816164
276.634162	8000.308801	12.484096	-0.056837	4.816163
276.437534	8000.290286	12.489101	-0.056800	4.816158
276.637423	8000.292850	12.494106	-0.056838	4.816158
276.611160	8000.275288	12.499111	-0.056833	4.816153
276.476364	8000.323065	12.504115	-0.056808	4.816168
276.454599	8000.300243	12.509120	-0.056804	4.816161
276.497237	8000.267905	12.514125	-0.056812	4.816151
276.491348	8000.305199	12.519130	-0.056811	4.816162
276.408361	8000.296223	12.524135	-0.056795	4.816160
276.721034	8000.298696	12.529139	-0.056854	4.816159
276.561367	8000.311834	12.534144	-0.056824	4.816164
276.386714	8000.302265	12.539149	-0.056792	4.816162
276.533750	8000.315623	12.544154	-0.056819	4.816165
276.479396	8000.254817	12.549159	-0.056809	4.816148
276.505586	8000.310854	12.554163	-0.056814	4.816164
276.549287	8000.304176	12.559168	-0.056822	4.816162
276.521541	8000.268425	12.564173	-0.056817	4.816151
276.384616	8000.303343	12.569178	-0.056792	4.816162
276.293625	8000.305975	12.574183	-0.056775	4.816163
276.310904	8000.273177	12.579187	-0.056778	4.816154
276.400614	8000.280153	12.584192	-0.056795	4.816155
276.295413	8000.300689	12.589197	-0.056775	4.816162
276.436636	8000.327830	12.594202	-0.056802	4.816169
276.380928	8000.272342	12.599207	-0.056792	4.816153
276.565664	8000.300272	12.604211	-0.056826	4.816160
276.571922	8000.280094	12.609216	-0.056827	4.816154
276.658671	8000.309453	12.614221	-0.056844	4.816163
276.583615	8000.340151	12.619226	-0.056830	4.816172
276.583762	8000.292085	12.624231	-0.056830	4.816158
276.626291	8000.335599	12.629235	-0.056838	4.816170
276.598396	8000.305187	12.634240	-0.056833	4.816162
276.406589	8000.339109	12.639245	-0.056797	4.816173
276.420197	8000.337227	12.644250	-0.056800	4.816172
276.429509	8000.312832	12.649255	-0.056801	4.816165
276.434270	8000.353524	12.654259	-0.056802	4.816177
276.443249	8000.319507	12.659264	-0.056804	4.816167
276.384090	8000.306691	12.664269	-0.056793	4.816163
276.605932	8000.324610	12.669274	-0.056835	4.816167
276.463606	8000.308148	12.674279	-0.056808	4.816163
276.476811	8000.339378	12.679283	-0.056811	4.816172
276.589098	8000.332875	12.684288	-0.056832	4.816170
276.612013	8000.306590	12.689293	-0.056836	4.816162
276.768681	8000.337216	12.694298	-0.056865	4.816170
276.576619	8000.294212	12.699303	-0.056830	4.816158
276.620612	8000.308906	12.704307	-0.056838	4.816163
276.539950	8000.302110	12.709312	-0.056823	4.816161
276.712699	8000.304182	12.714317	-0.056855	4.816161
276.648020	8000.311564	12.719322	-0.056843	4.816163
276.444080	8000.249114	12.724327	-0.056805	4.816146
276.526088	8000.300822	12.729331	-0.056821	4.816161
276.426702	8000.291550	12.734336	-0.056802	4.816158
276.525341	8000.307235	12.739341	-0.056821	4.816163
276.561347	8000.305759	12.744346	-0.056828	4.816162
276.410178	8000.270975	12.749351	-0.056799	4.816153
276.471150	8000.322302	12.754355	-0.056811	4.816167
276.381540	8000.297181	12.759360	-0.056794	4.816160
276.663188	8000.278792	12.764365	-0.056847	4.816153
276.583679	8000.301930	12.769370	-0.056832	4.816161
276.488384	8000.284185	12.774375	-0.056814	4.816156
276.569710	8000.313445	12.779379	-0.056830	4.816164
276.774109	8000.322502	12.784384	-0.056868	4.816166
276.491410	8000.336614	12.789389	-0.056815	4.816171
276.413555	8000.343757	12.794394	-0.056801	4.816174
276.588527	8000.302066	12.799399	-0.056833	4.816161
276.667368	8000.322735	12.804403	-0.056848	4.816166
276.467358	8000.312706	12.809408	-0.056811	4.816164
276.565540	8000.286716	12.814413	-0.056829	4.816156
276.618103	8000.337891	12.819418	-0.056839	4.816171
276.410083	8000.273230	12.824423	-0.056801	4.816153
276.455715	8000.298638	12.829427	-0.056809	4.816160
276.660431	8000.284196	12.834432	-0.056847	4.816155
276.499304	8000.257778	12.839437	-0.056817	4.816148
276.593123	8000.310769	12.844442	-0.056835	4.816163
276.573543	8000.277302	12.849447	-0.056831	4.816153
276.718655	8000.316266	12.854451	-0.056859	4.816164
276.524614	8000.307413	12.859456	-0.056823	4.816163
276.462626	8000.287067	12.864461	-0.056811	4.816157
276.693539	8000.325450	12.869466	-0.056854	4.816167
276.395575	8000.299756	12.874471	-0.056799	4.816161
276.397923	8000.348951	12.879475	-0.056799	4.816175
276.483295	8000.330208	12.884480	-0.056815	4.816169
276.595941	8000.266020	12.889485	-0.056836	4.816150
276.267140	8000.315621	12.894490	-0.056775	4.816166
276.357594	8000.282014	12.899495	-0.056792	4.816156
276.575596	8000.289179	12.904499	-0.056833	4.816157
276.350718	8000.310750	12.909504	-0.056791	4.816164
276.343552	8000.293535	12.914509	-0.056790	4.816159
276.452763	8000.312617	12.919514	-0.056810	4.816164
276.487538	8000.258769	12.924519	-0.056817	4.816148
276.703006	8000.286188	12.929523	-0.056857	4.816155
276.715937	8000.290704	12.934528	-0.056859	4.816157
276.754522	8000.248677	12.939533	-0.056867	4.816144
276.859987	8000.334998	12.944538	-0.056886	4.816169
276.715588	8000.304610	12.949543	-0.056860	4.816161
276.762616	8000.297992	12.954547	-0.056868	4.816158
276.558896	8000.314605	12.959552	-0.056831	4.816164
276.509696	8000.315858	12.964557	-0.056822	4.816165
276.720764	8000.305804	12.969562	-0.056861	4.816161
276.571862	8000.259309	12.974567	-0.056833	4.816148
276.520713	8000.308603	12.979571	-0.056824	4.816163
276.427023	8000.288750	12.984576	-0.056806	4.816158
276.435040	8000.289972	12.989581	-0.056808	4.816158
276.480234	8000.320713	12.994586	-0.056817	4.816167
276.506177	8000.237860	12.999591	-0.056821	4.816142
276.708712	8000.292821	13.004595	-0.056859	4.816157
276.763490	8000.317327	13.009600	-0.056870	4.816164
276.631276	8000.293570	13.014605	-0.056845	4.816158
276.578682	8000.299034	13.019610	-0.056835	4.816160
276.728726	8000.253687	13.024615	-0.056863	4.816146
276.624269	8000.308424	13.029619	-0.056844	4.816162
276.678407	8000.291251	13.034624	-0.056854	4.816157
276.727811	8000.264378	13.039629	-0.056863	4.816149
276.621652	8000.296648	13.044634	-0.056844	4.816159
276.559503	8000.284846	13.049639	-0.056832	4.816156
276.756065	8000.294828	13.054643	-0.056869	4.816158
276.747856	8000.313918	13.059648	-0.056867	4.816163
276.395608	8000.265873	13.064653	-0.056802	4.816151
276.674013	8000.298706	13.069658	-0.056854	4.816159
276.675776	8000.290199	13.074663	-0.056854	4.816157
276.595787	8000.293030	13.079667	-0.056839	4.816158
276.730256	8000.296545	13.084672	-0.056865	4.816158
276.668915	8000.233476	13.089677	-0.056853	4.816140
276.683227	8000.307460	13.094682	-0.056856	4.816162
276.498388	8000.289159	13.099687	-0.056822	4.816157
276.738100	8000.321292	13.104691	-0.056866	4.816165
276.849006	8000.297670	13.109696	-0.056887	4.816158
276.650331	8000.272708	13.114701	-0.056850	4.816152
276.591289	8000.323995	13.119706	-0.056839	4.816167
276.741460	8000.309632	13.124711	-0.056867	4.816162
276.809295	8000.331170	13.129715	-0.056880	4.816168
276.837458	8000.340235	13.134720	-0.056885	4.816170
276.728260	8000.335058	13.139725	-0.056865	4.816169
276.788831	8000.328686	13.144730	-0.056876	4.816167
276.600126	8000.284674	13.149735	-0.056841	4.816155
276.486800	8000.321088	13.154739	-0.056820	4.816167
276.510150	8000.290537	13.159744	-0.056825	4.816158
276.497909	8000.278571	13.164749	-0.056823	4.816154
276.695815	8000.316355	13.169754	-0.056860	4.816164
276.727959	8000.280622	13.174759	-0.056866	4.816153
276.688492	8000.270299	13.179763	-0.056858	4.816151
276.687262	8000.286310	13.184768	-0.056858	4.816155
276.637953	8000.281150	13.189773	-0.056849	4.816154
276.635664	8000.345219	13.194778	-0.056849	4.816173
276.532195	8000.274975	13.199783	-0.056830	4.816153
276.625101	8000.326881	13.204787	-0.056847	4.816168
276.677686	8000.319296	13.209792	-0.056857	4.816165
276.454270	8000.282133	13.214797	-0.056815	4.816155
276.771259	8000.346649	13.219802	-0.056874	4.816173
276.714589	8000.303963	13.224807	-0.056864	4.816160
276.664722	8000.308409	13.229811	-0.056855	4.816162
276.490190	8000.294568	13.234816	-0.056822	4.816159
276.572673	8000.315302	13.239821	-0.056838	4.816164
276.832069	8000.322151	13.244826	-0.056886	4.816165
276.622777	8000.261740	13.249831	-0.056847	4.816148
276.884988	8000.287871	13.254835	-0.056896	4.816155
276.759005	8000.287731	13.259840	-0.056873	4.816155
276.641903	8000.280273	13.264845	-0.056851	4.816154
276.639453	8000.308014	13.269850	-0.056851	4.816162
276.870707	8000.309011	13.274855	-0.056894	4.816161
276.929104	8000.280164	13.279859	-0.056905	4.816152
276.629273	8000.271529	13.284864	-0.056849	4.816151
276.784717	8000.270083	13.289869	-0.056878	4.816150
276.942755	8000.335991	13.294874	-0.056908	4.816168
276.718920	8000.306298	13.299879	-0.056866	4.816161
276.733700	8000.329010	13.304883	-0.056869	4.816168
276.885657	8000.328569	13.309888	-0.056897	4.816167
276.795421	8000.272453	13.314893	-0.056880	4.816151
276.739567	8000.325935	13.319898	-0.056870	4.816167
276.591804	8000.298691	13.324903	-0.056843	4.816159
276.714798	8000.309477	13.329907	-0.056866	4.816162
276.863330	8000.314315	13.334912	-0.056893	4.816163
276.792533	8000.303424	13.339917	-0.056880	4.816160
276.987265	8000.349698	13.344922	-0.056917	4.816172
276.874081	8000.315602	13.349927	-0.056896	4.816163
276.779392	8000.334192	13.354931	-0.056878	4.816169
276.879266	8000.289003	13.359936	-0.056897	4.816155
276.622315	8000.282215	13.364941	-0.056849	4.816154
276.714981	8000.260399	13.369946	-0.056866	4.816148
276.774298	8000.290329	13.374951	-0.056877	4.816156
276.599347	8000.276480	13.379955	-0.056845	4.816153
276.618093	8000.288580	13.384960	-0.056849	4.816156
276.798054	8000.266211	13.389965	-0.056882	4.816149
276.944457	8000.332976	13.394970	-0.056910	4.816168
276.664292	8000.289442	13.399975	-0.056857	4.816156
276.721177	8000.340695	13.404979	-0.056868	4.816171
276.811938	8000.316708	13.409984	-0.056885	4.816163
276.824790	8000.306265	13.414989	-0.056888	4.816160
276.811801	8000.313516	13.419994	-0.056885	4.816163
276.668087	8000.274594	13.424999	-0.056859	4.816152
276.793379	8000.295036	13.430003	-0.056882	4.816157
276.783021	8000.314087	13.435008	-0.056880	4.816163
276.825700	8000.255040	13.440013	-0.056888	4.816145
276.902615	8000.324819	13.445018	-0.056903	4.816165
276.823284	8000.281721	13.450023	-0.056888	4.816153
276.903077	8000.292792	13.455027	-0.056903	4.816156
277.025554	8000.308910	13.460032	-0.056926	4.816160
276.791840	8000.265150	13.465037	-0.056882	4.816148
276.847314	8000.330266	13.470042	-0.056893	4.816167
276.743280	8000.271764	13.475047	-0.056873	4.816151
276.834674	8000.291591	13.480051	-0.056890	4.816156
276.867084	8000.292187	13.485056	-0.056897	4.816156
276.622636	8000.253575	13.490061	-0.056851	4.816146
276.742075	8000.329466	13.495066	-0.056873	4.816168
276.700135	8000.292389	13.500071	-0.056866	4.816157
276.747069	8000.237693	13.505075	-0.056875	4.816141
277.039346	8000.326334	13.510080	-0.056929	4.816165
277.054777	8000.297776	13.515085	-0.056932	4.816157
277.020210	8000.324935	13.520090	-0.056926	4.816165
276.923013	8000.288992	13.525095	-0.056908	4.816155
277.042939	8000.285833	13.530099	-0.056930	4.816153
277.005512	8000.328965	13.535104	-0.056923	4.816166
276.763340	8000.306419	13.540109	-0.056878	4.816161
276.993961	8000.338387	13.545114	-0.056921	4.816169
276.822797	8000.342770	13.550119	-0.056889	4.816171
276.648889	8000.337487	13.555123	-0.056857	4.816170
276.629183	8000.302950	13.560128	-0.056854	4.816160
276.671981	8000.239632	13.565133	-0.056862	4.816142
276.719125	8000.267204	13.570138	-0.056870	4.816149
276.684789	8000.220650	13.575143	-0.056864	4.816136
276.902043	8000.306862	13.580147	-0.056905	4.816160
276.867798	8000.301975	13.585152	-0.056898	4.816159
276.893527	8000.287493	13.590157	-0.056903	4.816154
276.983158	8000.324382	13.595162	-0.056920	4.816165
276.965057	8000.280259	13.600167	-0.056917	4.816152
276.838083	8000.323904	13.605171	-0.056893	4.816165
276.801341	8000.321109	13.610176	-0.056886	4.816165
276.843679	8000.299449	13.615181	-0.056894	4.816158
276.977654	8000.301887	13.620186	-0.056919	4.816158
276.720209	8000.271585	13.625191	-0.056872	4.816151
276.694410	8000.256168	13.630195	-0.056867	4.816146
277.029481	8000.296440	13.635200	-0.056929	4.816156
276.788042	8000.281386	13.640205	-0.056884	4.816153
276.968362	8000.320989	13.645210	-0.056918	4.816164
276.817889	8000.319336	13.650215	-0.056890	4.816164
276.982151	8000.291340	13.655219	-0.056921	4.816155
277.006492	8000.344140	13.660224	-0.056925	4.816170
276.866760	8000.327725	13.665229	-0.056899	4.816166
276.897419	8000.349657	13.670234	-0.056905	4.816173
276.735075	8000.326421	13.675239	-0.056875	4.816167
276.998951	8000.355788	13.680243	-0.056924	4.816174
277.016204	8000.322989	13.685248	-0.056928	4.816164
276.920123	8000.327665	13.690253	-0.056910	4.816166
277.024630	8000.365893	13.695258	-0.056929	4.816177
276.779718	8000.332613	13.700263	-0.056884	4.816168
276.911769	8000.323264	13.705267	-0.056909	4.816165
276.841821	8000.346576	13.710272	-0.056896	4.816172
276.803448	8000.308495	13.715277	-0.056889	4.816161
276.787689	8000.335994	13.720282	-0.056886	4.816169
276.845671	8000.298593	13.725287	-0.056897	4.816158
276.686654	8000.275418	13.730291	-0.056867	4.816152
276.921909	8000.301060	13.735296	-0.056911	4.816158
277.006364	8000.327172	13.740301	-0.056927	4.816165
277.031604	8000.332980	13.745306	-0.056932	4.816167
277.038756	8000.311750	13.750311	-0.056933	4.816161
276.933719	8000.292759	13.755315	-0.056913	4.816156
276.877042	8000.304559	13.760320	-0.056903	4.816159
276.899456	8000.301769	13.765325	-0.056907	4.816158
277.003634	8000.351743	13.770330	-0.056927	4.816173
276.946739	8000.328283	13.775335	-0.056916	4.816166
276.885474	8000.341069	13.780339	-0.056905	4.816170
276.835113	8000.344437	13.785344	-0.056896	4.816171
276.648335	8000.303665	13.790349	-0.056861	4.816160
276.742712	8000.287222	13.795354	-0.056879	4.816155
276.770279	8000.294140	13.800359	-0.056884	4.816157
276.710750	8000.274906	13.805363	-0.056873	4.816152
276.876403	8000.305696	13.810368	-0.056904	4.816160
276.894772	8000.298559	13.815373	-0.056907	4.816158
276.961103	8000.323274	13.820378	-0.056920	4.816164
276.891570	8000.325226	13.825383	-0.056907	4.816165
277.097005	8000.322549	13.830387	-0.056945	4.816163
277.027304	8000.327704	13.835392	-0.056932	4.816165
276.869223	8000.314161	13.840397	-0.056903	4.816162
276.768202	8000.345456	13.845402	-0.056884	4.816172
276.874573	8000.345257	13.850407	-0.056904	4.816171
277.068950	8000.373363	13.855411	-0.056940	4.816178
276.905854	8000.362934	13.860416	-0.056910	4.816176
276.827549	8000.333744	13.865421	-0.056895	4.816168
277.114291	8000.372073	13.870426	-0.056949	4.816178
276.990273	8000.334575	13.875431	-0.056926	4.816168
276.780375	8000.350006	13.880435	-0.056887	4.816173
277.062009	8000.358328	13.885440	-0.056939	4.816174
276.863671	8000.297046	13.890445	-0.056903	4.816157
276.981257	8000.318417	13.895450	-0.056925	4.816163
276.894027	8000.316843	13.900455	-0.056908	4.816163
276.841665	8000.308423	13.905459	-0.056899	4.816161
276.888348	8000.347739	13.910464	-0.056908	4.816172
276.975078	8000.300175	13.915469	-0.056924	4.816158
277.093631	8000.330111	13.920474	-0.056946	4.816166
277.089784	8000.300134	13.925479	-0.056945	4.816157
276.788074	8000.326722	13.930483	-0.056889	4.816166
276.884655	8000.361601	13.935488	-0.056907	4.816176
276.833336	8000.316875	13.940493	-0.056898	4.816163
276.678822	8000.332243	13.945498	-0.056869	4.816168
276.755605	8000.319755	13.950503	-0.056883	4.816164
276.781616	8000.337328	13.955507	-0.056888	4.816169
276.951487	8000.360716	13.960512	-0.056920	4.816175
276.872048	8000.333643	13.965517	-0.056905	4.816168
276.956414	8000.355480	13.970522	-0.056921	4.816174
277.005825	8000.333948	13.975527	-0.056930	4.816167
276.913782	8000.352586	13.980531	-0.056913	4.816173
277.122268	8000.369196	13.985536	-0.056952	4.816177
276.905510	8000.331084	13.990541	-0.056912	4.816167
276.878042	8000.343415	13.995546	-0.056907	4.816171
276.938242	8000.315668	14.000551	-0.056918	4.816162
277.017836	8000.301094	14.005555	-0.056933	4.816158
277.070010	8000.336237	14.010560	-0.056943	4.816168
276.897719	8000.310684	14.015565	-0.056911	4.816161
277.075086	8000.363054	14.020570	-0.056944	4.816175
276.921185	8000.315399	14.025575	-0.056916	4.816162
276.897714	8000.308571	14.030579	-0.056911	4.816160
277.198636	8000.315105	14.035584	-0.056967	4.816161
277.221798	8000.323012	14.040589	-0.056972	4.816163
277.087942	8000.341960	14.045594	-0.056947	4.816169
276.917855	8000.315378	14.050599	-0.056915	4.816162
277.068011	8000.305289	14.055603	-0.056943	4.816158
277.039866	8000.331496	14.060608	-0.056938	4.816166
276.999992	8000.310482	14.065613	-0.056931	4.816160
277.143468	8000.345144	14.070618	-0.056958	4.816170
277.013129	8000.354540	14.075623	-0.056933	4.816173
277.106937	8000.320993	14.080627	-0.056951	4.816163
277.232577	8000.331826	14.085632	-0.056975	4.816165
277.118319	8000.320147	14.090637	-0.056953	4.816163
276.947054	8000.338416	14.095642	-0.056922	4.816169
276.896386	8000.317206	14.100647	-0.056912	4.816163
276.997360	8000.339344	14.105651	-0.056931	4.816169
277.132267	8000.367440	14.110656	-0.056956	4.816176
276.952049	8000.323581	14.115661	-0.056923	4.816164
277.110409	8000.364923	14.120666	-0.056952	4.816176
277.086129	8000.334576	14.125671	-0.056948	4.816167
276.832599	8000.331054	14.130675	-0.056901	4.816167
277.044449	8000.337041	14.135680	-0.056940	4.816168
277.226202	8000.333936	14.140685	-0.056974	4.816166
277.140225	8000.355888	14.145690	-0.056958	4.816173
277.229340	8000.330803	14.150695	-0.056975	4.816165
277.136174	8000.318438	14.155699	-0.056958	4.816162
277.230722	8000.320161	14.160704	-0.056975	4.816162
277.032905	8000.327264	14.165709	-0.056939	4.816165
277.244350	8000.328971	14.170714	-0.056978	4.816164
277.000041	8000.340573	14.175719	-0.056933	4.816169
276.899102	8000.333409	14.180723	-0.056914	4.816168
276.959535	8000.359085	14.185728	-0.056925	4.816175
277.061916	8000.338514	14.190733	-0.056944	4.816168
277.074933	8000.363331	14.195738	-0.056947	4.816175
276.772329	8000.316184	14.200743	-0.056891	4.816163
277.016756	8000.340924	14.205747	-0.056936	4.816169
276.977335	8000.355175	14.210752	-0.056929	4.816173
276.962190	8000.319651	14.215757	-0.056926	4.816163
276.952730	8000.359018	14.220762	-0.056925	4.816175
276.906771	8000.340030	14.225767	-0.056916	4.816169
276.999269	8000.343852	14.230771	-0.056933	4.816170
276.861928	8000.317865	14.235776	-0.056908	4.816163
277.069765	8000.257540	14.240781	-0.056947	4.816144
277.040187	8000.326456	14.245786	-0.056941	4.816165
276.935225	8000.301056	14.250791	-0.056922	4.816158
277.283870	8000.355465	14.255795	-0.056987	4.816172
277.181311	7999.381411	14.260800	-0.056967	4.815888

277.060223	7996.111563	14.265805	-0.056943	4.814933
277.152172	7990.628340	14.270810	-0.056956	4.813329
276.828365	7983.959049	14.275815	-0.056892	4.811381
276.753816	7976.629101	14.280819	-0.056873	4.809236
276.808806	7969.025323	14.285824	-0.056878	4.807010
276.730396	7961.189346	14.290829	-0.056859	4.804716
276.919382	7953.438395	14.295834	-0.056889	4.802444
276.856896	7945.379095	14.300839	-0.056872	4.800082
276.891962	7937.449935	14.305843	-0.056874	4.797756
276.770546	7929.423118	14.310848	-0.056846	4.795402
276.537526	7921.396363	14.315853	-0.056797	4.793047
276.598266	7913.362415	14.320858	-0.056804	4.790687
276.769541	7905.394704	14.325863	-0.056830	4.788345
276.616132	7897.369494	14.330867	-0.056797	4.785986
276.530307	7889.443791	14.335872	-0.056776	4.783655
276.483245	7881.431370	14.340877	-0.056762	4.781297
276.555697	7873.412004	14.345882	-0.056770	4.778936
276.383644	7865.436395	14.350887	-0.056733	4.776587
276.340093	7857.356527	14.355891	-0.056720	4.774206
276.381939	7849.451310	14.360896	-0.056722	4.771875
276.198361	7841.347834	14.365901	-0.056683	4.769485
276.187971	7833.396862	14.370906	-0.056676	4.767138
276.148439	7825.343721	14.375911	-0.056663	4.764760
276.164454	7817.415813	14.380915	-0.056661	4.762418
275.983675	7809.403629	14.385920	-0.056622	4.760050
276.022648	7801.391042	14.390925	-0.056625	4.757680
276.147574	7793.424703	14.395930	-0.056643	4.755322
276.126932	7785.341264	14.400935	-0.056634	4.752929
276.001182	7777.287976	14.405939	-0.056605	4.750544
275.793190	7769.355724	14.410944	-0.056561	4.748194
275.703818	7761.305780	14.415949	-0.056539	4.745808
275.754197	7753.387880	14.420954	-0.056544	4.743459
275.819675	7745.362596	14.425959	-0.056551	4.741077
275.792552	7737.364420	14.430963	-0.056541	4.738702
275.664165	7729.360701	14.435968	-0.056512	4.736324
275.676102	7721.340597	14.440973	-0.056509	4.733941
275.561379	7713.310534	14.445978	-0.056482	4.731553
275.466505	7705.327802	14.450983	-0.056459	4.729178
275.336251	7697.288983	14.455987	-0.056430	4.726785
275.618635	7689.313135	14.460992	-0.056477	4.724409
275.294714	7681.359017	14.465997	-0.056412	4.722039
275.287290	7673.383972	14.471002	-0.056406	4.719662
275.096651	7665.389160	14.476007	-0.056365	4.717277
275.084984	7657.316555	14.481011	-0.056358	4.714868
275.218512	7649.362366	14.486016	-0.056377	4.712493
275.077526	7641.268534	14.491021	-0.056346	4.710075
275.098476	7633.307799	14.496026	-0.056345	4.707695
274.790687	7625.303259	14.501031	-0.056282	4.705302
274.919526	7617.371428	14.506035	-0.056301	4.702929
275.031351	7609.338112	14.511040	-0.056317	4.700524
274.713346	7601.355284	14.516045	-0.056252	4.698133
274.709905	7593.305279	14.521050	-0.056247	4.695721
274.715411	7585.288641	14.526055	-0.056243	4.693317
274.662527	7577.240285	14.531059	-0.056228	4.690903
274.625018	7569.312689	14.536064	-0.056215	4.688524
274.482351	7561.257398	14.541069	-0.056184	4.686105
274.553463	7553.306563	14.546074	-0.056192	4.683716
274.689977	7545.360225	14.551079	-0.056212	4.681327
274.535828	7537.276850	14.556083	-0.056178	4.678896
274.715989	7529.337917	14.561088	-0.056207	4.676507
274.530438	7521.236822	14.566093	-0.056167	4.674069
274.453472	7513.167655	14.571098	-0.056148	4.671638
274.451862	7505.200531	14.576103	-0.056142	4.669237
274.428951	7497.211512	14.581107	-0.056133	4.666828
274.365873	7489.231581	14.586112	-0.056116	4.664421
274.141589	7481.261126	14.591117	-0.056069	4.662015
274.136655	7473.225758	14.596122	-0.056063	4.659588
274.080281	7465.298654	14.601127	-0.056047	4.657193
273.883171	7457.206689	14.606131	-0.056005	4.654747
273.991246	7449.249473	14.611136	-0.056020	4.652340
273.771293	7441.186583	14.616141	-0.055974	4.649900
273.768171	7433.247487	14.621146	-0.055969	4.647496
273.762033	7425.204321	14.626151	-0.055962	4.645060
273.669097	7417.274196	14.631155	-0.055940	4.642656
273.658032	7409.246638	14.636160	-0.055933	4.640221
273.676635	7401.253240	14.641165	-0.055931	4.637796
273.683678	7393.223892	14.646170	-0.055927	4.635358
273.505461	7385.220801	14.651175	-0.055889	4.632927
273.436195	7377.159660	14.656179	-0.055871	4.630478
273.433527	7369.240547	14.661184	-0.055865	4.628070
273.582151	7361.187448	14.666189	-0.055888	4.625620
273.449514	7353.245574	14.671194	-0.055858	4.623202
273.394880	7345.210722	14.676199	-0.055843	4.620755
273.348624	7337.222168	14.681203	-0.055829	4.618321
273.227692	7329.207009	14.686208	-0.055801	4.615877
273.196951	7321.187082	14.691213	-0.055790	4.613431
272.994286	7313.170173	14.696218	-0.055748	4.610984
272.974460	7305.190526	14.701223	-0.055739	4.608547
273.188624	7297.132595	14.706227	-0.055773	4.606085
273.227649	7289.224768	14.711232	-0.055776	4.603668
273.086370	7281.154646	14.716237	-0.055744	4.601200
272.855607	7273.216375	14.721242	-0.055696	4.598771
272.882240	7265.219242	14.726247	-0.055696	4.596322
272.865219	7257.104109	14.731251	-0.055688	4.593836
273.039746	7249.143032	14.736256	-0.055715	4.591396
272.618727	7241.116143	14.741261	-0.055631	4.588934
272.746660	7233.091371	14.746266	-0.055650	4.586472
272.879949	7225.153211	14.751271	-0.055670	4.584035
272.616085	7217.136301	14.756275	-0.055616	4.581572
272.498753	7209.132780	14.761280	-0.055589	4.579112
272.574615	7201.104926	14.766285	-0.055597	4.576644
272.580023	7193.168737	14.771290	-0.055593	4.574202
272.177774	7185.115845	14.776295	-0.055513	4.571723
272.319824	7177.084656	14.781299	-0.055535	4.569249
272.283023	7169.164501	14.786304	-0.055523	4.566808
272.147881	7161.137485	14.791309	-0.055492	4.564333
272.170674	7153.174172	14.796314	-0.055492	4.561877
272.236128	7145.163462	14.801319	-0.055499	4.559404
272.213500	7137.190690	14.806323	-0.055489	4.556942
272.134262	7129.149697	14.811328	-0.055469	4.554457
272.148740	7121.099696	14.816333	-0.055467	4.551968
272.069747	7113.085708	14.821338	-0.055447	4.549489
271.996416	7105.108376	14.826343	-0.055428	4.547020
271.984607	7097.068654	14.831347	-0.055421	4.544530
271.870900	7089.174792	14.836352	-0.055395	4.542084
271.810105	7081.103793	14.841357	-0.055378	4.539581
271.672555	7073.158364	14.846362	-0.055347	4.537117
271.603732	7065.120451	14.851367	-0.055329	4.534622
271.488398	7057.085214	14.856371	-0.055303	4.532126
271.818858	7049.086340	14.861376	-0.055359	4.529642
271.755498	7041.126947	14.866381	-0.055342	4.527167
271.470912	7033.094885	14.871386	-0.055284	4.524668
271.482814	7025.166986	14.876391	-0.055281	4.522201
271.539383	7017.119870	14.881395	-0.055287	4.519695
271.787372	7009.158186	14.886400	-0.055328	4.517215
271.562792	7001.092611	14.891405	-0.055281	4.514700
271.531750	6993.061396	14.896410	-0.055270	4.512195
271.547337	6985.046353	14.901415	-0.055268	4.509694
271.352688	6977.052192	14.906419	-0.055226	4.507197
271.350101	6969.072181	14.911424	-0.055221	4.504704
271.344200	6961.103610	14.916429	-0.055214	4.502213
271.233515	6953.087352	14.921434	-0.055189	4.499705
270.979045	6945.088680	14.926439	-0.055136	4.497202
270.908086	6937.062235	14.931443	-0.055118	4.494688
271.033565	6929.072611	14.936448	-0.055136	4.492185
270.822724	6921.041377	14.941453	-0.055092	4.489667
270.992493	6913.047360	14.946458	-0.055118	4.487160
271.023033	6905.063923	14.951463	-0.055119	4.484655
270.762821	6897.081540	14.956467	-0.055065	4.482147
270.810642	6889.086061	14.961472	-0.055069	4.479635
270.762933	6881.086006	14.966477	-0.055055	4.477120
270.705001	6873.042941	14.971482	-0.055039	4.474590
270.708463	6865.041552	14.976487	-0.055034	4.472072
270.404701	6857.023895	14.981491	-0.054973	4.469546
270.604659	6849.057383	14.986496	-0.055005	4.467037
270.480754	6841.023329	14.991501	-0.054977	4.464504
270.573049	6833.075755	14.996506	-0.054989	4.461997
270.425350	6825.065930	15.001511	-0.054956	4.459468
270.238298	6817.034454	15.006515	-0.054916	4.456931
270.307020	6809.040390	15.011520	-0.054924	4.454406
270.345486	6801.015640	15.016525	-0.054926	4.451869
270.368133	6793.019315	15.021530	-0.054925	4.449339
270.140615	6785.037327	15.026535	-0.054877	4.446812
269.920964	6777.000752	15.031539	-0.054831	4.444266
270.153777	6769.070837	15.036544	-0.054870	4.441754
270.022678	6761.018814	15.041549	-0.054840	4.439201
269.877517	6753.024784	15.046554	-0.054808	4.436664
270.014415	6745.021044	15.051559	-0.054828	4.434124
269.871779	6736.964472	15.056563	-0.054797	4.431565
269.885730	6729.004881	15.061568	-0.054794	4.429035
269.682225	6720.943737	15.066573	-0.054751	4.426471
269.839591	6712.990462	15.071578	-0.054775	4.423941
269.660581	6705.041318	15.076583	-0.054737	4.421410
269.555345	6697.002709	15.081587	-0.054712	4.418849
269.574698	6689.012128	15.086592	-0.054710	4.416302
269.505582	6680.975531	15.091597	-0.054692	4.413739
269.413425	6672.957660	15.096602	-0.054670	4.411180
269.388493	6664.992392	15.101607	-0.054660	4.408637
269.486007	6656.945920	15.106611	-0.054673	4.406067
269.412080	6648.996492	15.111616	-0.054654	4.403526
269.285830	6641.003684	15.116621	-0.054626	4.400969
269.148404	6633.030380	15.121626	-0.054595	4.398417
269.033040	6625.018538	15.126631	-0.054569	4.395851
269.032546	6616.987226	15.131635	-0.054563	4.393278
269.251809	6608.999010	15.136640	-0.054599	4.390718
269.213745	6600.998093	15.141645	-0.054587	4.388151
268.934847	6592.942580	15.146650	-0.054530	4.385564
269.130968	6585.009509	15.151655	-0.054561	4.383018
269.103200	6576.993396	15.156659	-0.054551	4.380442
268.992737	6569.056213	15.161664	-0.054525	4.377889
268.926071	6560.978413	15.166669	-0.054508	4.375290
269.026368	6552.997593	15.171674	-0.054521	4.372722
268.803012	6544.994116	15.176679	-0.054474	4.370143
268.606455	6537.021137	15.181683	-0.054433	4.367572
268.678500	6528.983313	15.186688	-0.054441	4.364980
268.470097	6520.989142	15.191693	-0.054397	4.362400
268.580685	6512.994959	15.196698	-0.054412	4.359819
268.641359	6505.054696	15.201703	-0.054419	4.357255
268.476678	6496.963961	15.206707	-0.054383	4.354638
268.572327	6488.904154	15.211712	-0.054395	4.352032
268.450457	6480.902455	15.216717	-0.054368	4.349442
268.439574	6472.919838	15.221722	-0.054360	4.346857
268.246002	6464.909878	15.226727	-0.054319	4.344260
268.247911	6456.977984	15.231731	-0.054315	4.341689
268.299123	6449.001719	15.236736	-0.054319	4.339101
268.237562	6440.969947	15.241741	-0.054302	4.336494
268.004265	6432.969560	15.246746	-0.054254	4.333894
267.959261	6424.952962	15.251751	-0.054240	4.331288
268.284258	6416.905785	15.256755	-0.054296	4.328674
268.039342	6408.969158	15.261760	-0.054245	4.326090
267.918452	6400.994523	15.266765	-0.054217	4.323492
267.867872	6392.938945	15.271770	-0.054203	4.320868
267.971849	6384.999891	15.276775	-0.054217	4.318280
267.682188	6376.942933	15.281779	-0.054158	4.315651
267.868115	6368.920856	15.286784	-0.054187	4.313034
267.616976	6360.891168	15.291789	-0.054135	4.310410
267.788360	6352.929736	15.296794	-0.054162	4.307809
267.800104	6344.934606	15.301799	-0.054159	4.305195
267.770634	6336.963388	15.306803	-0.054149	4.302587
267.748289	6328.954912	15.311808	-0.054139	4.299965
267.715088	6320.979217	15.316813	-0.054128	4.297352
267.708605	6312.929695	15.321818	-0.054122	4.294714
267.512960	6304.905709	15.326823	-0.054080	4.292081
267.276152	6296.898160	15.331827	-0.054031	4.289451
267.433069	6288.923381	15.336832	-0.054055	4.286834
267.372889	6280.946246	15.341837	-0.054039	4.284212
267.283399	6272.967136	15.346842	-0.054017	4.281588
267.057007	6264.947896	15.351847	-0.053970	4.278948
267.031227	6256.947766	15.356851	-0.053960	4.276315
267.055821	6248.934286	15.361856	-0.053959	4.273675
266.926756	6240.869911	15.366861	-0.053930	4.271016
266.955542	6232.893734	15.371866	-0.053930	4.268386
266.871111	6224.913974	15.376871	-0.053909	4.265752
266.808191	6216.911229	15.381875	-0.053892	4.263109
266.712056	6208.921888	15.386880	-0.053869	4.260468
266.682272	6200.920730	15.391885	-0.053859	4.257823
266.663523	6192.902580	15.396890	-0.053850	4.255170
266.554571	6184.915378	15.401895	-0.053825	4.252525
266.558910	6176.872733	15.406899	-0.053820	4.249861
266.685440	6168.942060	15.411904	-0.053839	4.247233
266.377183	6160.891440	15.416909	-0.053776	4.244561
266.343267	6152.970289	15.421914	-0.053765	4.241932
266.299553	6144.921815	15.426919	-0.053752	4.239259
266.183820	6136.970583	15.431923	-0.053725	4.236615
266.269558	6128.935273	15.436928	-0.053736	4.233945
266.209773	6120.882778	15.441933	-0.053719	4.231265
266.104199	6112.895759	15.446938	-0.053695	4.228605
266.122734	6104.944051	15.451943	-0.053693	4.225956
266.092427	6096.920063	15.456947	-0.053682	4.223281
266.283283	6088.956625	15.461952	-0.053713	4.220627
266.007107	6080.961981	15.466957	-0.053656	4.217956
265.852163	6072.911076	15.471962	-0.053622	4.215266
266.034465	6064.951755	15.476967	-0.053651	4.212608
265.711893	6056.888990	15.481971	-0.053586	4.209909
265.934398	6048.970286	15.486976	-0.053622	4.207261
265.600393	6040.918277	15.491981	-0.053555	4.204562
265.673994	6032.974907	15.496986	-0.053563	4.201901
265.703084	6024.979235	15.501991	-0.053564	4.199221
265.514345	6016.935720	15.506995	-0.053523	4.196521
265.668600	6008.920480	15.512000	-0.053547	4.193832
265.432386	6000.847975	15.517005	-0.053498	4.191118
265.665779	5992.857300	15.522010	-0.053536	4.188435
265.498169	5984.892470	15.527015	-0.053500	4.185754
265.326190	5976.910698	15.532019	-0.053463	4.183066
265.421295	5968.923878	15.537024	-0.053475	4.180377
265.459118	5960.910636	15.542029	-0.053477	4.177677
265.155236	5952.912526	15.547034	-0.053415	4.174977
265.089393	5944.921343	15.552039	-0.053398	4.172280
265.081897	5936.884490	15.557043	-0.053391	4.169566
265.228333	5928.955042	15.562048	-0.053414	4.166889
264.958214	5920.921451	15.567053	-0.053358	4.164170
264.888649	5912.930925	15.572058	-0.053340	4.161466
264.939756	5904.939799	15.577063	-0.053344	4.158761
264.822724	5896.910612	15.582067	-0.053318	4.156040
264.840132	5888.876723	15.587072	-0.053316	4.153317
264.696987	5880.875582	15.592077	-0.053284	4.150602
264.756880	5872.904144	15.597082	-0.053290	4.147897
264.788921	5864.880943	15.602087	-0.053291	4.145172
264.743475	5856.945556	15.607091	-0.053277	4.142475
264.822732	5848.935821	15.612096	-0.053287	4.139752
264.643244	5840.906348	15.617101	-0.053248	4.137017
264.386636	5832.919775	15.622106	-0.053195	4.134295
264.714728	5824.871413	15.627111	-0.053251	4.131556
264.578391	5816.863817	15.632115	-0.053221	4.128824
264.552821	5808.886022	15.637120	-0.053211	4.126102
264.501628	5800.886085	15.642125	-0.053196	4.123369
264.254104	5792.908548	15.647130	-0.053145	4.120641
264.203591	5784.953969	15.652135	-0.053130	4.117921
264.316563	5776.877434	15.657139	-0.053146	4.115159
264.346204	5768.881330	15.662144	-0.053147	4.112422
264.042754	5760.864453	15.667149	-0.053085	4.109672
263.985328	5752.871350	15.672154	-0.053069	4.106931
263.975996	5744.880018	15.677159	-0.053062	4.104189
263.869893	5736.879446	15.682163	-0.053037	4.101442
263.905881	5728.918961	15.687168	-0.053039	4.098708
263.800224	5720.910984	15.692173	-0.053014	4.095954
263.785066	5712.922270	15.697178	-0.053006	4.093206
263.841918	5704.869106	15.702183	-0.053012	4.090435
263.778501	5696.918391	15.707187	-0.052995	4.087696
263.715380	5688.913263	15.712192	-0.052978	4.084936
263.646429	5680.941855	15.717197	-0.052960	4.082186
263.577868	5672.941477	15.722202	-0.052942	4.079424
263.584030	5665.006905	15.727207	-0.052938	4.076683
263.445836	5656.916246	15.732211	-0.052907	4.073885
263.511803	5648.900803	15.737216	-0.052914	4.071114
263.350214	5640.922324	15.742221	-0.052879	4.068351
263.292920	5632.906451	15.747226	-0.052863	4.065574
263.112292	5624.985658	15.752231	-0.052825	4.062827
262.931250	5616.936224	15.757235	-0.052786	4.060033
263.139345	5608.980178	15.762240	-0.052819	4.057275
263.199206	5600.935696	15.767245	-0.052825	4.054482
263.207981	5592.890731	15.772250	-0.052822	4.051687
263.186157	5584.927963	15.777255	-0.052813	4.048918
263.027788	5576.890160	15.782259	-0.052778	4.046119
263.025208	5568.968085	15.787264	-0.052772	4.043360
262.793755	5560.942678	15.792269	-0.052724	4.040560
262.987960	5552.973246	15.797274	-0.052755	4.037784
262.813541	5544.947714	15.802279	-0.052718	4.034981
262.615667	5536.826934	15.807283	-0.052676	4.032143
262.643704	5528.877486	15.812288	-0.052676	4.029365
262.610775	5520.891472	15.817293	-0.052664	4.026572
262.403858	5512.929135	15.822298	-0.052621	4.023783
262.524352	5504.941467	15.827303	-0.052638	4.020988
262.545262	5496.947559	15.832307	-0.052637	4.018187
262.211378	5488.928260	15.837312	-0.052570	4.015370
262.266121	5480.923673	15.842317	-0.052575	4.012562
262.425338	5472.860572	15.847322	-0.052599	4.009734
262.385967	5464.948570	15.852327	-0.052587	4.006953
262.316751	5456.880976	15.857331	-0.052569	4.004115
262.318171	5448.946394	15.862336	-0.052564	4.001323
262.394839	5440.920073	15.867341	-0.052573	3.998498
262.260060	5432.938930	15.872346	-0.052543	3.995683
262.080523	5424.915915	15.877351	-0.052504	3.992851
261.932931	5416.868055	15.882355	-0.052472	3.990009
262.105243	5408.933521	15.887360	-0.052499	3.987210
261.951275	5400.895642	15.892365	-0.052465	3.984367
261.918822	5392.938349	15.897370	-0.052454	3.981552
261.967387	5384.954779	15.902375	-0.052457	3.978728
261.813897	5376.937671	15.907379	-0.052424	3.975886
261.777842	5368.961462	15.912384	-0.052412	3.973059
261.411188	5360.941141	15.917389	-0.052339	3.970209
261.666479	5352.936514	15.922394	-0.052381	3.967372
261.797101	5344.952119	15.927399	-0.052400	3.964539
261.551691	5336.976966	15.932403	-0.052349	3.961700
261.409467	5328.989620	15.937408	-0.052318	3.958857
261.363007	5320.992152	15.942413	-0.052304	3.956010
261.449141	5312.948612	15.947418	-0.052315	3.953146
261.390675	5304.930896	15.952423	-0.052299	3.950287
261.202491	5296.938350	15.957427	-0.052259	3.947433
261.412059	5288.965778	15.962432	-0.052293	3.944591
261.250284	5281.002811	15.967437	-0.052257	3.941744
261.302396	5273.001261	15.972442	-0.052262	3.938884
260.953441	5265.036358	15.977447	-0.052192	3.936029
261.000369	5256.974367	15.982451	-0.052195	3.933143
261.033217	5248.967751	15.987456	-0.052196	3.930275
260.766470	5241.003484	15.992461	-0.052142	3.927415
260.730215	5232.979816	15.997466	-0.052130	3.924536
260.846560	5225.002293	16.002471	-0.052146	3.921674
260.847989	5217.012825	16.007475	-0.052141	3.918803
260.863989	5209.029356	16.012480	-0.052139	3.915933
260.755623	5200.986868	16.017485	-0.052114	3.913037
260.630229	5192.981577	16.022490	-0.052085	3.910152
260.693599	5185.019468	16.027495	-0.052092	3.907283
260.695881	5176.951196	16.032499	-0.052087	3.904374
260.652946	5168.979449	16.037504	-0.052074	3.901496
260.412325	5161.013359	16.042509	-0.052024	3.898614
260.351957	5153.022422	16.047514	-0.052008	3.895725
260.539525	5145.003089	16.052519	-0.052038	3.892828
260.320964	5136.946879	16.057523	-0.051992	3.889907
260.259216	5129.013588	16.062528	-0.051975	3.887032
260.340643	5121.012445	16.067533	-0.051985	3.884133
260.317099	5113.002099	16.072538	-0.051976	3.881227
260.233688	5105.037877	16.077543	-0.051955	3.878333
260.261078	5097.018825	16.082547	-0.051955	3.875420
260.250986	5088.818106	16.087552	-0.051948	3.872438
259.984572	5080.856025	16.092557	-0.051893	3.869536
260.000412	5072.918407	16.097562	-0.051891	3.866645
260.039335	5064.942672	16.102567	-0.051893	3.863739
259.869183	5056.940520	16.107571	-0.051856	3.860817
259.791209	5048.979722	16.112576	-0.051837	3.857910
259.697256	5040.995926	16.117581	-0.051814	3.854992
259.617106	5032.975641	16.122586	-0.051794	3.852059
259.925972	5024.986371	16.127591	-0.051846	3.849142
259.775223	5017.017087	16.132595	-0.051813	3.846221
259.839866	5009.013144	16.137600	-0.051820	3.843290
259.439481	5001.034094	16.142605	-0.051741	3.840356
259.599511	4993.045648	16.147610	-0.051765	3.837428
259.609278	4985.039281	16.152615	-0.051762	3.834488
259.413487	4976.997002	16.157619	-0.051720	3.831529
259.461778	4969.024608	16.162624	-0.051724	3.828597
259.521939	4961.028811	16.167629	-0.051730	3.825656
259.353102	4953.085069	16.172634	-0.051694	3.822726
259.205163	4945.091291	16.177639	-0.051661	3.819776
259.025434	4937.115710	16.182643	-0.051622	3.816830
259.279955	4929.076892	16.187648	-0.051665	3.813867
259.226410	4921.060098	16.192653	-0.051650	3.810904
259.030582	4913.058556	16.197658	-0.051608	3.807940
259.134882	4905.094165	16.202663	-0.051622	3.804995
259.133481	4897.104918	16.207667	-0.051617	3.802036
259.054521	4889.141536	16.212672	-0.051597	3.799083
258.841349	4881.124870	16.217677	-0.051552	3.796104
258.751361	4873.078845	16.222682	-0.051530	3.793115
258.914159	4865.055522	16.227687	-0.051555	3.790138
258.585105	4857.085726	16.232691	-0.051489	3.787167
258.732513	4849.080902	16.237696	-0.051511	3.784192
258.619945	4841.108545	16.242701	-0.051485	3.781220
258.461137	4833.076588	16.247706	-0.051451	3.778223
258.520724	4825.125123	16.252711	-0.051457	3.775258
258.445688	4817.080899	16.257715	-0.051437	3.772254
258.388829	4809.105520	16.262720	-0.051422	3.769273
258.382064	4801.084234	16.267725	-0.051415	3.766274
258.265057	4793.115175	16.272730	-0.051388	3.763289
258.297836	4785.135956	16.277735	-0.051389	3.760301
258.119273	4777.134234	16.282739	-0.051351	3.757298
258.262765	4769.125255	16.287744	-0.051373	3.754298
258.138929	4761.094022	16.292749	-0.051344	3.751280
257.884277	4753.087278	16.297754	-0.051292	3.748266
258.075247	4745.098771	16.302759	-0.051322	3.745267
257.855332	4737.115327	16.307763	-0.051276	3.742257
257.797208	4729.126765	16.312768	-0.051260	3.739247
257.882929	4721.163912	16.317773	-0.051271	3.736248
257.682909	4713.147402	16.322778	-0.051229	3.733219
257.825116	4705.108731	16.327783	-0.051250	3.730188
257.795829	4697.145072	16.332787	-0.051240	3.727178
257.906665	4689.109756	16.337792	-0.051255	3.724142
257.854067	4681.181936	16.342797	-0.051240	3.721141
257.623740	4673.216548	16.347802	-0.051192	3.718119
257.532541	4665.216833	16.352807	-0.051170	3.715084
257.467330	4657.105244	16.357811	-0.051153	3.712005
257.308284	4649.148584	16.362816	-0.051118	3.708980
257.326315	4641.131339	16.367821	-0.051116	3.705934
257.333733	4633.174700	16.372826	-0.051112	3.702908
257.170557	4625.192894	16.377831	-0.051077	3.699866
256.987055	4617.210031	16.382835	-0.051038	3.696821
257.199820	4609.214764	16.387840	-0.051072	3.693778
256.987996	4601.179922	16.392845	-0.051028	3.690706
256.832996	4593.220083	16.397850	-0.050994	3.687663
256.948868	4585.220643	16.402855	-0.051010	3.684608
257.063627	4577.224602	16.407859	-0.051026	3.681552
257.038512	4569.251670	16.412864	-0.051016	3.678499
257.032828	4561.243371	16.417869	-0.051010	3.675431
256.690212	4553.233901	16.422874	-0.050941	3.672351
256.977112	4545.218090	16.427879	-0.050990	3.669281
256.748088	4537.224437	16.432883	-0.050942	3.666205
256.756145	4529.257528	16.437888	-0.050938	3.663142
256.785904	4521.220408	16.442893	-0.050939	3.660051
256.687839	4513.258601	16.447898	-0.050915	3.656982
256.841388	4505.258284	16.452903	-0.050939	3.653902
256.651367	4497.244111	16.457907	-0.050898	3.650806
256.613169	4489.288809	16.462912	-0.050886	3.647734
256.364647	4481.267263	16.467917	-0.050835	3.644628
256.240052	4473.325749	16.472922	-0.050806	3.641553
256.295506	4465.312620	16.477927	-0.050811	3.638453
256.090416	4457.299945	16.482931	-0.050768	3.635343
256.309729	4449.245010	16.487936	-0.050804	3.632226
256.120913	4441.261140	16.492941	-0.050764	3.629123
255.906116	4433.252236	16.497946	-0.050718	3.626006
255.871642	4425.310905	16.502951	-0.050707	3.622918
255.796686	4417.281318	16.507955	-0.050688	3.619792
255.906228	4409.338842	16.512960	-0.050703	3.616702
255.804599	4401.317743	16.517965	-0.050679	3.613574
255.683130	4393.276230	16.522970	-0.050651	3.610433
255.721393	4385.339281	16.527975	-0.050653	3.607336
255.507174	4377.337443	16.532979	-0.050608	3.604203
255.638582	4369.382930	16.537984	-0.050628	3.601096
255.441233	4361.411432	16.542989	-0.050586	3.597970
255.445885	4353.376880	16.547994	-0.050581	3.594823
255.457608	4345.365578	16.552999	-0.050579	3.591681
255.373211	4337.353824	16.558003	-0.050558	3.588535
255.355431	4329.350734	16.563008	-0.050549	3.585391
255.095145	4321.426827	16.568013	-0.050496	3.582268
255.193492	4313.412013	16.573018	-0.050509	3.579117
255.231822	4305.425974	16.578023	-0.050511	3.575973
255.159711	4297.369428	16.583027	-0.050492	3.572795
255.090102	4289.383975	16.588032	-0.050474	3.569642
255.268197	4281.406584	16.593037	-0.050502	3.566497
255.200332	4273.416962	16.598042	-0.050484	3.563337
255.141110	4265.435409	16.603047	-0.050468	3.560178
255.095488	4257.452884	16.608051	-0.050455	3.557016
255.108858	4249.412520	16.613056	-0.050452	3.553830
254.967850	4241.362408	16.618061	-0.050421	3.550633
254.637220	4233.386277	16.623066	-0.050354	3.547457
254.646977	4225.412672	16.628071	-0.050351	3.544289
254.507976	4217.410160	16.633075	-0.050320	3.541102
254.681550	4209.399504	16.638080	-0.050347	3.537918
254.590405	4201.436879	16.643085	-0.050325	3.534742
254.626313	4193.424222	16.648090	-0.050326	3.531548
254.561855	4185.456818	16.653095	-0.050309	3.528366
254.546217	4177.425796	16.658099	-0.050301	3.525157
254.454467	4169.478848	16.663104	-0.050279	3.521976
254.358476	4161.493447	16.668109	-0.050256	3.518777
254.134773	4153.514129	16.673114	-0.050209	3.515573
254.173727	4145.499672	16.678119	-0.050211	3.512361
254.013442	4137.507708	16.683123	-0.050176	3.509148
254.085473	4129.503851	16.688128	-0.050185	3.505935
254.112252	4121.524737	16.693133	-0.050184	3.502727
253.840269	4113.537083	16.698138	-0.050129	3.499504
254.074370	4105.561364	16.703143	-0.050167	3.496299
253.881794	4097.535990	16.708147	-0.050126	3.493057
253.736658	4089.519905	16.713152	-0.050094	3.489817
253.648410	4081.567952	16.718157	-0.050072	3.486602
253.670620	4073.569261	16.723162	-0.050071	3.483369
253.832167	4065.596437	16.728167	-0.050096	3.480147
253.610287	4057.635451	16.733171	-0.050050	3.476915
253.552366	4049.589097	16.738176	-0.050034	3.473651
253.561055	4041.561257	16.743181	-0.050031	3.470393
253.331177	4033.609659	16.748186	-0.049983	3.467155
253.417202	4025.612286	16.753191	-0.049993	3.463906
253.218031	4017.622698	16.758195	-0.049951	3.460648
253.335553	4009.653161	16.763200	-0.049968	3.457405
253.320493	4001.614346	16.768205	-0.049960	3.454127
253.187262	3993.602527	16.773210	-0.049930	3.450853
253.297201	3985.643886	16.778215	-0.049946	3.447605
253.035321	3977.643864	16.783219	-0.049892	3.444325
252.879422	3969.678916	16.788224	-0.049857	3.441059
252.883958	3961.722409	16.793229	-0.049853	3.437800
253.091335	3953.634588	16.798234	-0.049887	3.434490
252.983581	3945.664324	16.803239	-0.049861	3.431215
252.773636	3937.661401	16.808243	-0.049817	3.427919
252.657326	3929.680673	16.813248	-0.049790	3.424633
252.771486	3921.691175	16.818253	-0.049807	3.421348
252.802034	3913.713097	16.823258	-0.049807	3.418061
252.793618	3905.736792	16.828263	-0.049800	3.414771
252.689524	3897.716321	16.833267	-0.049776	3.411456
252.808529	3889.712544	16.838272	-0.049793	3.408152
252.899993	3881.717991	16.843277	-0.049805	3.404848
252.701870	3873.788233	16.848282	-0.049763	3.401558
252.705006	3865.790109	16.853287	-0.049758	3.398243
252.347743	3857.810893	16.858291	-0.049687	3.394920
252.341661	3849.736819	16.863296	-0.049680	3.391567
252.403943	3841.711578	16.868301	-0.049687	3.388233
252.345225	3833.720820	16.873306	-0.049671	3.384906
252.259490	3825.821873	16.878311	-0.049650	3.381613
252.076411	3817.807861	16.883315	-0.049611	3.378265
251.946149	3809.831086	16.888320	-0.049581	3.374931
251.989325	3801.837920	16.893325	-0.049584	3.371594
251.898816	3793.813213	16.898330	-0.049562	3.368235
251.944557	3785.843160	16.903335	-0.049565	3.364900
251.761407	3777.894470	16.908339	-0.049526	3.361563
251.868251	3769.877003	16.913344	-0.049541	3.358204
251.980502	3761.864076	16.918349	-0.049557	3.354844
251.804145	3753.853366	16.923354	-0.049519	3.351471
251.731453	3745.887911	16.928359	-0.049500	3.348117
251.623065	3737.866855	16.933363	-0.049475	3.344735
251.661418	3729.911654	16.938368	-0.049477	3.341383
251.679781	3721.934350	16.943373	-0.049475	3.338018
251.556754	3713.933728	16.948378	-0.049447	3.334634
251.429168	3705.948328	16.953383	-0.049418	3.331253
251.311300	3697.926023	16.958387	-0.049391	3.327853
251.480416	3689.916448	16.963392	-0.049418	3.324465
251.215916	3682.006506	16.968397	-0.049363	3.321101
251.068484	3674.002600	16.973402	-0.049331	3.317697
251.194121	3666.012416	16.978407	-0.049349	3.314306
251.111362	3657.959179	16.983411	-0.049328	3.310877
251.078261	3649.977365	16.988416	-0.049317	3.307476
250.984581	3642.005465	16.993421	-0.049294	3.304074
251.023177	3634.018429	16.998426	-0.049297	3.300667
251.129817	3626.059159	17.003431	-0.049311	3.297271
250.734088	3618.067291	17.008435	-0.049232	3.293839
250.830758	3610.029913	17.013440	-0.049245	3.290402
250.833404	3602.059520	17.018445	-0.049241	3.286986
250.659794	3594.072439	17.023450	-0.049203	3.283553
250.625485	3586.121281	17.028455	-0.049192	3.280137
250.827160	3578.105699	17.033459	-0.049224	3.276699
250.631477	3570.100115	17.038464	-0.049183	3.273247
250.418232	3562.111903	17.043469	-0.049138	3.269797
250.328541	3554.100801	17.048474	-0.049116	3.266339
250.417684	3546.140580	17.053479	-0.049127	3.262906
250.259412	3538.142561	17.058483	-0.049093	3.259444
250.319867	3530.175058	17.063488	-0.049099	3.255999
250.251936	3522.159217	17.068493	-0.049081	3.252525
249.937568	3514.162976	17.073498	-0.049018	3.249046
250.123175	3506.180010	17.078503	-0.049047	3.245588
250.083727	3498.185175	17.083507	-0.049034	3.242113
250.006755	3490.222472	17.088512	-0.049015	3.238647
250.040597	3482.238775	17.093517	-0.049016	3.235172
249.927688	3474.161938	17.098522	-0.048990	3.231647
249.991790	3466.185573	17.103527	-0.048997	3.228169
249.810087	3458.197708	17.108531	-0.048958	3.224673
249.739642	3450.263917	17.113536	-0.048940	3.221200
249.840483	3442.270027	17.118541	-0.048953	3.217705
249.527585	3434.272829	17.123546	-0.048890	3.214187
249.551133	3426.303580	17.128551	-0.048889	3.210692
249.479804	3418.300741	17.133555	-0.048871	3.207174
249.325031	3410.335845	17.138560	-0.048837	3.203666
249.341233	3402.339565	17.143565	-0.048835	3.200146
249.432509	3394.361286	17.148570	-0.048847	3.196634
249.594014	3386.363171	17.153575	-0.048872	3.193113
249.330444	3378.322196	17.158579	-0.048817	3.189551
249.352173	3370.348667	17.163584	-0.048816	3.186026
249.304037	3362.403284	17.168589	-0.048802	3.182507
249.242256	3354.404640	17.173594	-0.048786	3.178960
249.148986	3346.450317	17.178599	-0.048763	3.175428
249.004242	3338.441667	17.183603	-0.048731	3.171865
249.023663	3330.424252	17.188608	-0.048730	3.168301
248.988923	3322.454000	17.193613	-0.048718	3.164752
248.770550	3314.501275	17.198618	-0.048672	3.161199
248.740998	3306.500930	17.203623	-0.048662	3.157629
248.651763	3298.509129	17.208627	-0.048640	3.154056
248.549570	3290.476744	17.213632	-0.048616	3.150460
248.625706	3282.505292	17.218637	-0.048625	3.146895
248.505873	3274.505490	17.223642	-0.048597	3.143304
248.413154	3266.543546	17.228647	-0.048575	3.139728
248.360794	3258.562470	17.233651	-0.048560	3.136141
248.363667	3250.571971	17.238656	-0.048555	3.132548
248.512312	3242.543092	17.243661	-0.048578	3.128940
248.530031	3234.554946	17.248666	-0.048576	3.125340
248.524046	3226.632955	17.253671	-0.048570	3.121765
248.176041	3218.666039	17.258675	-0.048500	3.118150
248.225082	3210.636215	17.263680	-0.048504	3.114521
248.123964	3202.663663	17.268685	-0.048480	3.110906
248.207375	3194.634645	17.273690	-0.048490	3.107270
248.034085	3186.690671	17.278695	-0.048453	3.103657
247.864157	3178.699400	17.283699	-0.048416	3.100018
247.871732	3170.735560	17.288704	-0.048413	3.096395
247.937522	3162.725901	17.293709	-0.048420	3.092749
247.624593	3154.730045	17.298714	-0.048356	3.089089
247.705453	3146.756264	17.303719	-0.048366	3.085452
247.574142	3138.794740	17.308723	-0.048337	3.081807
247.572268	3130.805808	17.313728	-0.048331	3.078151
247.710164	3122.786391	17.318733	-0.048352	3.074483
247.489239	3114.709370	17.323738	-0.048305	3.070767
247.304162	3106.787380	17.328743	-0.048266	3.067120
247.245448	3098.803055	17.333747	-0.048250	3.063446
247.483554	3090.783251	17.338752	-0.048289	3.059765
247.566778	3082.859830	17.343757	-0.048299	3.056116
247.184506	3074.862860	17.348762	-0.048223	3.052408
247.249291	3066.878708	17.353767	-0.048230	3.048721
247.072610	3058.900596	17.358771	-0.048192	3.045022
247.023841	3050.941369	17.363776	-0.048178	3.041333
247.220558	3042.957832	17.368781	-0.048209	3.037640
246.920536	3034.971925	17.373786	-0.048148	3.033918
246.923094	3026.966751	17.378791	-0.048144	3.030196
246.978755	3018.961898	17.383795	-0.048149	3.026473
246.933189	3010.986061	17.388800	-0.048135	3.022754
246.760159	3003.035306	17.393805	-0.048098	3.019036
246.732743	2995.038552	17.398810	-0.048088	3.015298
246.759677	2987.037395	17.403815	-0.048088	3.011557
246.715341	2979.046947	17.408819	-0.048074	3.007812
246.599083	2971.066013	17.413824	-0.048048	3.004064
246.612903	2963.106723	17.418829	-0.048045	3.000328
246.472179	2955.154983	17.423834	-0.048014	2.996582
246.409451	2947.134794	17.428839	-0.047997	2.992804
246.363952	2939.109712	17.433843	-0.047983	2.989020
246.376232	2931.126405	17.438848	-0.047980	2.985253
246.374835	2923.188292	17.443853	-0.047975	2.981502
246.063447	2915.201348	17.448858	-0.047912	2.977708
246.163658	2907.222549	17.453863	-0.047926	2.973934
245.981019	2899.210236	17.458867	-0.047886	2.970124
246.023375	2891.234256	17.463872	-0.047889	2.966338
245.872983	2883.275232	17.468877	-0.047856	2.962546
245.790656	2875.308062	17.473882	-0.047836	2.958748
245.793642	2867.330245	17.478887	-0.047831	2.954945
245.937858	2859.286758	17.483891	-0.047853	2.951113
245.800139	2851.329648	17.488896	-0.047822	2.947303
245.823503	2843.353166	17.493901	-0.047821	2.943486
245.530686	2835.382073	17.498906	-0.047762	2.939651
245.879412	2827.404201	17.503911	-0.047821	2.935841
245.631484	2819.392676	17.508915	-0.047770	2.931979
245.549722	2811.421153	17.513920	-0.047750	2.928139
245.566381	2803.444251	17.518925	-0.047748	2.924297
245.364765	2795.471838	17.523930	-0.047705	2.920441
245.510566	2787.521905	17.528935	-0.047727	2.916609
245.223255	2779.474853	17.533939	-0.047668	2.912702
245.328902	2771.440188	17.538944	-0.047683	2.908816
245.282167	2763.491457	17.543949	-0.047669	2.904959
245.116938	2755.527133	17.548954	-0.047633	2.901083
245.070418	2747.569463	17.553959	-0.047620	2.897211
244.901973	2739.588481	17.558963	-0.047583	2.893316
245.055718	2731.569316	17.563968	-0.047607	2.889414
245.019456	2723.607483	17.568973	-0.047595	2.885525
244.970668	2715.646305	17.573978	-0.047581	2.881630
244.878425	2707.690544	17.578983	-0.047558	2.877731
244.883507	2699.690242	17.583987	-0.047554	2.873809
244.905553	2691.686257	17.588992	-0.047553	2.869881
244.887527	2683.716095	17.593997	-0.047545	2.865963
244.496201	2675.761184	17.599002	-0.047467	2.862025
244.386272	2667.820729	17.604007	-0.047441	2.858105
244.454825	2659.792826	17.609011	-0.047449	2.854147
244.214524	2651.810103	17.614016	-0.047399	2.850188
244.269373	2643.842562	17.619021	-0.047404	2.846247
244.162685	2635.867106	17.624026	-0.047379	2.842288
244.239536	2627.908486	17.629031	-0.047388	2.838342
244.107108	2619.921804	17.634035	-0.047358	2.834365
243.942673	2611.910546	17.639040	-0.047323	2.830368
243.930797	2603.934679	17.644045	-0.047315	2.826392
243.857207	2595.948936	17.649050	-0.047296	2.822402
243.846850	2587.988542	17.654055	-0.047289	2.818422
243.627451	2580.007162	17.659059	-0.047243	2.814415
243.599306	2572.016650	17.664064	-0.047233	2.810407
243.822361	2564.023075	17.669069	-0.047269	2.806408
243.671072	2556.058272	17.674074	-0.047236	2.802395
243.674882	2548.106967	17.679079	-0.047232	2.798392
243.526900	2540.147998	17.684083	-0.047199	2.794371
243.485404	2532.124645	17.689088	-0.047186	2.790318
243.478350	2524.148482	17.694093	-0.047180	2.786284
243.292475	2516.177450	17.699098	-0.047140	2.782237
243.460325	2508.222653	17.704103	-0.047166	2.778213
243.270248	2500.254488	17.709107	-0.047126	2.774156
243.224426	2492.246961	17.714112	-0.047112	2.770081
243.012621	2484.311612	17.719117	-0.047068	2.766026
243.081427	2476.323474	17.724122	-0.047075	2.761956
242.983649	2468.369592	17.729127	-0.047052	2.757887
243.035885	2460.347742	17.734131	-0.047056	2.753786
242.962866	2452.303785	17.739136	-0.047038	2.749660
243.002071	2444.329893	17.744141	-0.047040	2.745571
242.897722	2436.367140	17.749146	-0.047015	2.741473
242.872499	2428.432486	17.754151	-0.047006	2.737388
242.660674	2420.465135	17.759155	-0.046961	2.733268
242.656801	2412.463573	17.764160	-0.046955	2.729138
242.376149	2404.527417	17.769165	-0.046898	2.725018
242.447194	2396.550861	17.774170	-0.046906	2.720892
242.418648	2388.599998	17.779175	-0.046896	2.716767
242.316382	2380.596114	17.784179	-0.046871	2.712604
242.426871	2372.585213	17.789184	-0.046887	2.708444
242.464441	2364.614422	17.794189	-0.046889	2.704294
242.030042	2356.690159	17.799194	-0.046803	2.700132
241.939048	2348.751555	17.804199	-0.046781	2.695978
242.133053	2340.704618	17.809203	-0.046812	2.691778
242.061676	2332.737721	17.814208	-0.046793	2.687598
241.891972	2324.802224	17.819213	-0.046757	2.683421
241.878855	2316.829450	17.824218	-0.046749	2.679228
242.076540	2308.846079	17.829223	-0.046781	2.675036
241.923530	2300.826442	17.834227	-0.046747	2.670796
241.804053	2292.874611	17.839232	-0.046720	2.666587
241.925467	2284.886128	17.844237	-0.046737	2.662368
241.785784	2276.943732	17.849242	-0.046706	2.658149
241.667212	2268.980306	17.854247	-0.046679	2.653914
241.572109	2260.980740	17.859251	-0.046656	2.649655
241.478369	2253.033462	17.864256	-0.046634	2.645416
241.395048	2245.088341	17.869261	-0.046613	2.641173
241.428989	2237.099047	17.874266	-0.046614	2.636907
241.306333	2229.119720	17.879271	-0.046586	2.632629
241.118783	2221.140747	17.884275	-0.046546	2.628339
241.200243	2213.152544	17.889280	-0.046556	2.624056
241.221115	2205.192053	17.894285	-0.046555	2.619777
241.198768	2197.229040	17.899290	-0.046546	2.615486
241.197558	2189.260012	17.904295	-0.046540	2.611186
240.987703	2181.306283	17.909299	-0.046496	2.606874
241.012305	2173.342802	17.914304	-0.046496	2.602565
241.005898	2165.383974	17.919309	-0.046489	2.598249
240.817997	2157.370497	17.924314	-0.046449	2.593884
240.883674	2149.236094	17.929319	-0.046456	2.589463
240.827952	2141.280086	17.934323	-0.046441	2.585123
240.668741	2133.392975	17.939328	-0.046406	2.580807
240.711569	2125.446786	17.944333	-0.046409	2.576465
240.622310	2117.469022	17.949338	-0.046387	2.572089
240.520651	2109.523780	17.954343	-0.046363	2.567723
240.555934	2101.547639	17.959347	-0.046365	2.563341
240.476417	2093.616003	17.964352	-0.046345	2.558969
240.309090	2085.682462	17.969357	-0.046308	2.554582
239.993174	2077.701810	17.974362	-0.046245	2.550151
240.108225	2069.712512	17.979367	-0.046261	2.545738
240.117119	2061.753263	17.984371	-0.046257	2.541326
240.018897	2053.791655	17.989376	-0.046234	2.536898
240.145317	2045.809830	17.994381	-0.046252	2.532467
240.093549	2037.824565	17.999386	-0.046238	2.528013
239.826197	2029.906038	18.004391	-0.046183	2.523573
239.704597	2021.961791	18.009395	-0.046155	2.519122
239.730027	2013.986398	18.014400	-0.046155	2.514656
239.672563	2005.981587	18.019405	-0.046139	2.510159
239.488352	1998.014070	18.024410	-0.046099	2.505666
239.454248	1990.079318	18.029415	-0.046088	2.501194
239.703953	1982.068898	18.034419	-0.046129	2.496692
239.630755	1974.090938	18.039424	-0.046111	2.492177
239.672228	1966.127817	18.044429	-0.046113	2.487670
239.485916	1958.184355	18.049434	-0.046073	2.483150
239.430916	1950.268920	18.054439	-0.046058	2.478647
239.200381	1942.325476	18.059443	-0.046010	2.474107
239.525806	1934.268227	18.064448	-0.046065	2.469534
239.375006	1926.343298	18.069453	-0.046032	2.464994
239.242232	1918.395574	18.074458	-0.046003	2.460433
239.199485	1910.452548	18.079463	-0.045989	2.455874
239.058502	1902.485027	18.084467	-0.045958	2.451284
238.929846	1894.513564	18.089472	-0.045929	2.446684
239.111196	1886.548981	18.094477	-0.045958	2.442103
238.996840	1878.601060	18.099482	-0.045931	2.437501
238.845742	1870.633993	18.104487	-0.045898	2.432876
238.777581	1862.616681	18.109491	-0.045880	2.428219
238.560113	1854.667463	18.114496	-0.045835	2.423582
238.610584	1846.723391	18.119501	-0.045839	2.418959
238.364080	1838.776265	18.124506	-0.045788	2.414303
238.519305	1830.783430	18.129511	-0.045812	2.409642
238.627311	1822.808485	18.134515	-0.045827	2.404979
238.302838	1814.899713	18.139520	-0.045761	2.400312
238.356249	1806.968737	18.144525	-0.045766	2.395652
238.529662	1798.929183	18.149530	-0.045793	2.390929
238.523286	1790.976653	18.154535	-0.045787	2.386233
238.249728	1783.064383	18.159539	-0.045731	2.381531
238.377759	1775.094198	18.164544	-0.045750	2.376817
238.283504	1767.151651	18.169549	-0.045727	2.372093
238.059387	1759.186059	18.174554	-0.045680	2.367334
237.892197	1751.265846	18.179559	-0.045644	2.362598
237.835249	1743.323293	18.184563	-0.045628	2.357848
237.904049	1735.321747	18.189568	-0.045636	2.353063
237.995954	1727.343701	18.194573	-0.045648	2.348285
237.810869	1719.386303	18.199578	-0.045608	2.343486
237.748288	1711.458770	18.204583	-0.045592	2.338706
237.491701	1703.525970	18.209587	-0.045539	2.333896
237.503122	1695.541088	18.214592	-0.045536	2.329068
237.525428	1687.582330	18.219597	-0.045535	2.324246
237.401648	1679.654808	18.224602	-0.045507	2.319420
237.501126	1671.690883	18.229607	-0.045520	2.314581
237.372480	1663.724045	18.234611	-0.045491	2.309712
237.310340	1655.752749	18.239616	-0.045474	2.304834
237.163883	1647.859539	18.244621	-0.045442	2.299987
237.105222	1639.889982	18.249626	-0.045426	2.295091
237.413435	1631.877476	18.254631	-0.045478	2.290188
237.250421	1623.969183	18.259635	-0.045443	2.285299
236.916380	1616.062326	18.264640	-0.045376	2.280386
236.905332	1608.119643	18.269645	-0.045368	2.275468
236.768867	1600.066176	18.274650	-0.045338	2.270460
236.796167	1592.117758	18.279655	-0.045338	2.265519
236.703562	1584.190480	18.284659	-0.045315	2.260571
236.582717	1576.255313	18.289664	-0.045288	2.255605
236.571841	1568.308228	18.294669	-0.045281	2.250630
236.620404	1560.332916	18.299674	-0.045285	2.245631
236.427517	1552.419088	18.304679	-0.045244	2.240639
236.410851	1544.471979	18.309683	-0.045235	2.235630
236.397197	1536.503002	18.314688	-0.045228	2.230596
236.531983	1528.541362	18.319693	-0.045248	2.225568
236.361161	1520.618254	18.324698	-0.045211	2.220527
236.165417	1512.704968	18.329703	-0.045169	2.215477
236.259016	1504.721529	18.334707	-0.045182	2.210398
236.203804	1496.784595	18.339712	-0.045166	2.205323
236.162031	1488.877700	18.344717	-0.045153	2.200257
235.810962	1480.962885	18.349722	-0.045083	2.195146
235.668791	1472.990234	18.354727	-0.045051	2.190005
235.563901	1465.032573	18.359731	-0.045027	2.184865
235.520015	1457.093025	18.364736	-0.045014	2.179730
235.661843	1449.132890	18.369741	-0.045035	2.174586
235.580303	1441.172978	18.374746	-0.045015	2.169410
235.484008	1433.244502	18.379751	-0.044992	2.164241
235.466278	1425.317392	18.384755	-0.044983	2.159067
235.435146	1417.379241	18.389760	-0.044972	2.153873
235.395328	1409.430093	18.394765	-0.044960	2.148657
235.236336	1401.495455	18.399770	-0.044925	2.143428
235.307851	1393.564343	18.404775	-0.044933	2.138210
235.103381	1385.644133	18.409779	-0.044890	2.132960
234.993564	1377.686646	18.414784	-0.044865	2.127681
235.114055	1369.752300	18.419789	-0.044882	2.122426
235.100669	1361.818788	18.424794	-0.044874	2.117147
234.806665	1353.872780	18.429799	-0.044815	2.111818
234.735625	1345.892024	18.434803	-0.044796	2.106475
234.790525	1337.947316	18.439808	-0.044801	2.101154
234.739695	1330.045847	18.444813	-0.044787	2.095838
234.487752	1322.125770	18.449818	-0.044735	2.090477
234.472709	1314.186754	18.454823	-0.044727	2.085112
234.489279	1306.250221	18.459827	-0.044725	2.079739
234.282123	1298.356129	18.464832	-0.044681	2.074358
234.448116	1290.370633	18.469837	-0.044707	2.068938
234.322110	1282.442768	18.474842	-0.044678	2.063513
234.317935	1274.535123	18.479847	-0.044673	2.058101
234.320060	1266.593724	18.484851	-0.044668	2.052652
234.013453	1258.678014	18.489856	-0.044606	2.047174
233.887014	1250.791422	18.494861	-0.044577	2.041721
233.795632	1242.859085	18.499866	-0.044555	2.036224
233.963880	1234.872984	18.504871	-0.044581	2.030702
233.765455	1226.962169	18.509875	-0.044539	2.025180
233.594592	1219.050673	18.514880	-0.044502	2.019645
233.588345	1211.128670	18.519885	-0.044496	2.014104
233.588008	1203.172000	18.524890	-0.044491	2.008524
233.539100	1195.260336	18.529895	-0.044477	2.002955
233.415891	1187.364227	18.534899	-0.044449	1.997374
233.440432	1179.418093	18.539904	-0.044448	1.991758
233.285043	1171.509610	18.544909	-0.044414	1.986133
233.141300	1163.596909	18.549914	-0.044382	1.980490
233.190198	1155.675549	18.554919	-0.044386	1.974846
233.241722	1147.722330	18.559923	-0.044391	1.969163
233.002136	1139.819799	18.564928	-0.044341	1.963468
233.106516	1131.907594	18.569933	-0.044356	1.957787
233.150814	1123.938008	18.574938	-0.044359	1.952042
233.011826	1116.014323	18.579943	-0.044328	1.946293
232.631606	1108.157195	18.584947	-0.044252	1.940549
232.496160	1100.231605	18.589952	-0.044222	1.934765
232.551071	1092.306507	18.594957	-0.044227	1.928984
232.368897	1084.393327	18.599962	-0.044188	1.923169
232.466114	1076.484141	18.604967	-0.044201	1.917370
232.432041	1068.555339	18.609971	-0.044189	1.911524
232.398921	1060.623858	18.614976	-0.044178	1.905659
232.366251	1052.735855	18.619981	-0.044167	1.899808
232.391741	1044.818271	18.624986	-0.044167	1.893923
232.180525	1036.923966	18.629991	-0.044122	1.888010
232.123996	1029.018954	18.634995	-0.044107	1.882089
232.070547	1021.116979	18.640000	-0.044092	1.876151
232.003007	1013.199129	18.645005	-0.044074	1.870181
231.758344	1005.302859	18.650010	-0.044023	1.864187
231.772839	997.404922	18.655015	-0.044021	1.858203
231.896799	989.467470	18.660019	-0.044039	1.852182
231.618945	981.585324	18.665024	-0.043982	1.846137
231.637975	973.694283	18.670029	-0.043981	1.840100
231.479744	965.811839	18.675034	-0.043946	1.834029
231.415190	957.894070	18.680039	-0.043929	1.827921
231.255434	950.020654	18.685043	-0.043894	1.821816
231.111547	942.134116	18.690048	-0.043862	1.815682
231.139217	934.214613	18.695053	-0.043863	1.809522
231.033985	926.317192	18.700058	-0.043838	1.803343
231.172853	918.416703	18.705063	-0.043859	1.797169
231.241641	910.463867	18.710067	-0.043866	1.790924
230.740527	902.611011	18.715072	-0.043768	1.784667
230.929590	894.710674	18.720077	-0.043798	1.778435
231.045530	886.789165	18.725082	-0.043815	1.772154
230.988889	878.908754	18.730087	-0.043799	1.765863
230.753509	871.076878	18.735091	-0.043750	1.759567
230.653574	863.193105	18.740096	-0.043727	1.753222
230.587156	855.299046	18.745101	-0.043709	1.746851
230.324421	847.438497	18.750106	-0.043655	1.740458
230.267215	839.577154	18.755111	-0.043639	1.734067
230.451136	831.649072	18.760115	-0.043669	1.727629
230.373746	823.761040	18.765120	-0.043649	1.721166
230.413855	815.895578	18.770125	-0.043652	1.714713
230.278459	808.000861	18.775130	-0.043621	1.708188
230.316218	800.118149	18.780135	-0.043623	1.701671
230.034232	792.293648	18.785139	-0.043566	1.695135
229.783664	784.430124	18.790144	-0.043514	1.688545
229.745028	776.570126	18.795149	-0.043502	1.681960
229.773930	768.687929	18.800154	-0.043502	1.675340
229.836451	760.789002	18.805159	-0.043509	1.668684
229.736200	752.927983	18.810163	-0.043485	1.662012
229.636093	745.078035	18.815168	-0.043461	1.655322
229.716125	737.198739	18.820173	-0.043471	1.648604
229.672896	729.340882	18.825178	-0.043458	1.641860
229.422411	721.528431	18.830183	-0.043406	1.635099
229.161182	713.634351	18.835187	-0.043353	1.628238
229.150418	705.760275	18.840192	-0.043346	1.621400
229.122480	697.919963	18.845197	-0.043335	1.614560
229.074228	690.045467	18.850202	-0.043321	1.607658
229.112946	682.195600	18.855207	-0.043324	1.600760
229.117466	674.348617	18.860211	-0.043319	1.593830
228.923607	666.502785	18.865216	-0.043278	1.586843
228.857218	658.682841	18.870221	-0.043261	1.579866
228.642267	650.860120	18.875226	-0.043216	1.572834
228.670792	642.996009	18.880231	-0.043216	1.565768
228.529180	635.200458	18.885235	-0.043185	1.558708
228.391614	627.349519	18.890240	-0.043154	1.551565
228.452328	619.487659	18.895245	-0.043160	1.544409
228.267205	611.668429	18.900250	-0.043121	1.537222
228.158801	603.846523	18.905255	-0.043096	1.530011
228.160668	596.008905	18.910259	-0.043091	1.522767
228.091195	588.186727	18.915264	-0.043073	1.515492
228.068223	580.357145	18.920269	-0.043064	1.508182
228.108463	572.514131	18.925274	-0.043066	1.500834
228.117009	564.706795	18.930279	-0.043063	1.493478
227.773013	556.927037	18.935283	-0.042994	1.486057
227.692547	549.131712	18.940288	-0.042974	1.478626
227.760551	541.275563	18.945293	-0.042981	1.471121
227.406045	533.481976	18.950298	-0.042910	1.463572
227.644823	525.636985	18.955303	-0.042950	1.456028
227.370899	517.867019	18.960307	-0.042894	1.448436
227.389762	510.053806	18.965312	-0.042892	1.440808
227.377152	502.280359	18.970317	-0.042885	1.433174
227.013059	494.508590	18.975322	-0.042812	1.425443
227.041736	486.720891	18.980327	-0.042813	1.417719
227.000871	478.928791	18.985331	-0.042800	1.409937
226.751622	471.167292	18.990336	-0.042749	1.402107
226.785842	463.390183	18.995341	-0.042750	1.394265
226.504020	455.616141	19.000346	-0.042693	1.386328
226.581808	447.831399	19.005351	-0.042702	1.378396
226.545379	440.044271	19.010355	-0.042690	1.370396
226.515952	432.270313	19.015360	-0.042680	1.362364
226.229756	424.570815	19.020365	-0.042622	1.354317
226.166510	416.795976	19.025370	-0.042605	1.346182
226.126871	409.050292	19.030375	-0.042592	1.338032
226.123680	401.288084	19.035379	-0.042587	1.329821
225.906060	393.561905	19.040384	-0.042541	1.321559
226.150085	385.759447	19.045389	-0.042582	1.313247
226.125581	377.918704	19.050394	-0.042572	1.304791
225.737193	370.262000	19.055399	-0.042495	1.296414
225.778511	362.522783	19.060403	-0.042498	1.287971
225.569638	354.834941	19.065408	-0.042454	1.279483
225.418516	347.144367	19.070413	-0.042421	1.270946
225.149725	339.464691	19.075418	-0.042366	1.262341
225.148787	331.747278	19.080423	-0.042361	1.253685
225.089732	324.047283	19.085427	-0.042345	1.244977
224.941415	316.367411	19.090432	-0.042312	1.236214
224.997982	308.646400	19.095437	-0.042318	1.227381
224.971539	300.951825	19.100442	-0.042308	1.218498
224.896685	293.282274	19.105447	-0.042289	1.209569
224.857065	285.613457	19.110451	-0.042277	1.200582
224.814287	277.952615	19.115456	-0.042264	1.191536
224.611176	270.321392	19.120461	-0.042221	1.182424
224.357862	262.703415	19.125466	-0.042169	1.173246
224.277829	255.061426	19.130471	-0.042149	1.164002
224.218860	247.430631	19.135475	-0.042134	1.154703
223.817322	239.810958	19.140480	-0.042054	1.145269
223.817314	232.179547	19.145485	-0.042049	1.135828
223.726754	224.551216	19.150490	-0.042027	1.126292
223.585704	216.969360	19.155495	-0.041996	1.116722
223.323949	209.397897	19.160499	-0.041943	1.107056
223.111507	201.823990	19.165504	-0.041898	1.097313
222.909063	194.264353	19.170509	-0.041856	1.087503
222.452862	186.753045	19.175514	-0.041766	1.077610
222.021961	179.225533	19.180519	-0.041681	1.067609
221.560353	171.720911	19.185523	-0.041590	1.057537
221.108381	164.202750	19.190528	-0.041501	1.047352
220.833909	156.701778	19.195533	-0.041445	1.037131
220.526903	149.188118	19.200538	-0.041383	1.026784
220.171228	141.709768	19.205543	-0.041312	1.016368
219.821156	134.236136	19.210547	-0.041242	1.005853
219.406479	126.784915	19.215552	-0.041160	0.995241
218.881893	119.332153	19.220557	-0.041058	0.984486
218.343486	111.913135	19.225562	-0.040953	0.973657
218.013878	104.476181	19.230567	-0.040887	0.962733
217.642337	97.073602	19.235571	-0.040813	0.951723
217.182551	89.684723	19.240576	-0.040722	0.940582
216.740697	82.318434	19.245581	-0.040635	0.929346
216.332942	74.963088	19.250586	-0.040555	0.917999
215.726821	67.639025	19.255591	-0.040437	0.906503
215.203883	60.564994	19.260595	-0.040335	0.895277