Tue Mar 23 11:04:21 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.576282	-0.015104	0.000000	-0.000013	0.722380

0.665015	-0.033810	0.005005	-0.000029	0.722375
0.563560	-0.015837	0.010010	-0.000010	0.722375
0.686832	-0.034294	0.015014	-0.000033	0.722382
0.592667	-0.021791	0.020019	-0.000016	0.722374
0.572438	-0.014384	0.025024	-0.000012	0.722381
0.559467	-0.013792	0.030029	-0.000010	0.722378
0.606275	-0.023683	0.035034	-0.000019	0.722375
0.539629	-0.009642	0.040038	-0.000006	0.722380
0.477760	-0.003723	0.045043	0.000005	0.722370
0.478160	0.000568	0.050048	0.000005	0.722378
0.524816	-0.008899	0.055053	-0.000004	0.722376
0.677516	-0.037045	0.060058	-0.000033	0.722375
0.720346	-0.040784	0.065062	-0.000041	0.722382
0.608299	-0.172852	0.070067	-0.000020	0.722084
0.686859	-0.186608	0.075072	-0.000034	0.722085
0.682130	-0.186689	0.080077	-0.000034	0.722083
0.548398	-0.164399	0.085082	-0.000009	0.722080
0.603811	-0.169387	0.090086	-0.000019	0.722090
0.585567	-0.171470	0.095091	-0.000016	0.722080
0.457435	-0.179371	0.100096	0.000008	0.722019
0.437276	-0.310608	0.105101	0.000012	0.721755
0.289515	-0.286693	0.110106	0.000039	0.721750
0.435596	-0.309175	0.115110	0.000012	0.721757
0.403784	-0.309119	0.120115	0.000018	0.721746
0.379983	-0.300880	0.125120	0.000022	0.721754
0.478218	-0.437984	0.130125	0.000004	0.721519
0.465363	-0.475313	0.135130	0.000006	0.721442
0.652151	-0.503735	0.140134	-0.000029	0.721451
0.481628	-0.478306	0.145139	0.000003	0.721442
0.573197	-0.563228	0.150144	-0.000014	0.721307
0.544541	-0.648195	0.155149	-0.000009	0.721130
0.440434	-0.631176	0.160154	0.000010	0.721127
0.443712	-0.626532	0.165158	0.000009	0.721138
0.314872	-0.687731	0.170163	0.000033	0.720972
0.442830	-0.752242	0.175168	0.000010	0.720890
0.154202	-0.702370	0.180173	0.000063	0.720887
0.198087	-0.722049	0.185178	0.000055	0.720864
0.212126	-0.884051	0.190182	0.000052	0.720550
0.045528	-0.858401	0.195187	0.000083	0.720543
0.012551	-0.849051	0.200192	0.000089	0.720550
0.287842	-1.007059	0.205197	0.000038	0.720335
0.077380	-1.023798	0.210202	0.000077	0.720229
0.143650	-1.031803	0.215206	0.000065	0.720236
0.093817	-1.128272	0.220211	0.000074	0.720029
0.202680	-1.208814	0.225216	0.000054	0.719909
0.381553	-1.242890	0.230221	0.000020	0.719904
0.293639	-1.349989	0.235226	0.000037	0.719663
0.426454	-1.399417	0.240230	0.000012	0.719612
0.098761	-1.374210	0.245235	0.000073	0.719547
0.133303	-1.517256	0.250240	0.000066	0.719277
0.127840	-1.517479	0.255245	0.000067	0.719275
-0.037052	-1.587781	0.260250	0.000098	0.719078
-0.047414	-1.641200	0.265254	0.000100	0.718969
-0.029779	-1.667525	0.270259	0.000096	0.718924
-0.095555	-1.795475	0.275264	0.000109	0.718648
-0.181898	-1.780742	0.280269	0.000125	0.718647
-0.211261	-1.881570	0.285274	0.000130	0.718438
-0.135419	-1.932508	0.290278	0.000116	0.718364
-0.218474	-1.988060	0.295283	0.000131	0.718225
-0.237470	-2.085893	0.300288	0.000135	0.718026
-0.075807	-2.143167	0.305293	0.000105	0.717970
-0.070598	-2.277729	0.310298	0.000104	0.717706
-0.191493	-2.260946	0.315302	0.000126	0.717696
-0.713312	-2.328595	0.320307	0.000223	0.717379
-2.624683	-1.985298	0.325312	0.000579	0.717385
-2.076628	-2.155507	0.330317	0.000477	0.717241
-3.041807	-2.063196	0.335322	0.000656	0.717084
-3.030534	-2.060796	0.340326	0.000654	0.717093
-3.252694	-2.106665	0.345331	0.000695	0.716924
-3.701630	-2.108144	0.350336	0.000779	0.716763
-3.763033	-2.100648	0.355341	0.000790	0.716757
-4.362805	-2.017575	0.360346	0.000902	0.716710
-4.603301	-2.103124	0.365350	0.000947	0.716456
-4.541116	-2.118425	0.370355	0.000935	0.716447
-5.098432	-2.015987	0.375360	0.001038	0.716454
-4.667190	-2.161518	0.380365	0.000958	0.716318
-5.486082	-2.108180	0.385370	0.001111	0.716135
-5.345606	-2.129072	0.390374	0.001084	0.716143
-5.990461	-2.020810	0.395379	0.001204	0.716130
-5.893376	-2.091359	0.400384	0.001186	0.716025
-6.466089	-2.060207	0.405389	0.001293	0.715885
-6.653592	-2.027334	0.410394	0.001327	0.715884
-6.340979	-2.079201	0.415398	0.001269	0.715892
-6.425287	-2.069708	0.420403	0.001285	0.715881
-7.116250	-2.104898	0.425408	0.001413	0.715567
-7.276345	-2.085524	0.430413	0.001443	0.715549
-7.489419	-2.050968	0.435418	0.001483	0.715543
-7.363786	-2.067805	0.440422	0.001459	0.715554
-7.895459	-1.977802	0.445427	0.001558	0.715545
-7.743828	-2.142137	0.450432	0.001530	0.715272
-8.284804	-2.064792	0.455437	0.001630	0.715235
-8.862729	-1.965918	0.460442	0.001738	0.715227
-8.262551	-2.067280	0.465446	0.001626	0.715238
-8.238656	-2.076463	0.470451	0.001621	0.715229
-8.590195	-2.082296	0.475456	0.001687	0.715093
-9.431996	-2.023637	0.480461	0.001843	0.714912
-9.034055	-2.097239	0.485466	0.001769	0.714907
-9.252692	-2.053863	0.490470	0.001810	0.714916
-9.698710	-1.979658	0.495475	0.001893	0.714906
-9.339464	-2.040235	0.500480	0.001826	0.714912
-9.174972	-2.125370	0.505485	0.001795	0.714802
-10.455597	-1.995973	0.510490	0.002033	0.714606
-9.840807	-2.102895	0.515494	0.001919	0.714611
-10.349072	-2.016617	0.520499	0.002013	0.714603
-10.411108	-2.003376	0.525504	0.002025	0.714608
-9.907050	-2.092146	0.530509	0.001931	0.714610
-10.155750	-2.077449	0.535514	0.001977	0.714551
-10.972210	-2.065887	0.540518	0.002129	0.714285
-11.041094	-2.057987	0.545523	0.002142	0.714277
-11.329601	-2.003661	0.550528	0.002195	0.714283
-10.979137	-2.067982	0.555533	0.002130	0.714279
-11.253073	-2.022339	0.560538	0.002181	0.714273
-10.996304	-2.062508	0.565542	0.002133	0.714284
-10.965715	-2.178448	0.570547	0.002127	0.714065
-12.157059	-2.012974	0.575552	0.002349	0.713972
-12.067857	-2.026949	0.580557	0.002332	0.713976
-11.961956	-2.048885	0.585562	0.002313	0.713970
-11.854344	-2.065747	0.590566	0.002292	0.713975
-12.137030	-2.018268	0.595571	0.002345	0.713970
-12.023929	-2.038150	0.600576	0.002324	0.713970
-12.684366	-2.077651	0.605581	0.002447	0.713658
-13.334624	-1.966577	0.610586	0.002568	0.713649
-13.221027	-1.982152	0.615590	0.002546	0.713658
-13.080744	-2.010526	0.620595	0.002520	0.713652
-13.096918	-2.006084	0.625600	0.002523	0.713655
-12.919530	-2.036947	0.630605	0.002490	0.713656
-12.980698	-2.029357	0.635610	0.002501	0.713650
-13.489350	-2.016729	0.640614	0.002596	0.713495
-14.490545	-1.905673	0.645619	0.002782	0.713361
-13.929023	-2.004259	0.650624	0.002678	0.713364
-13.731792	-2.040148	0.655629	0.002641	0.713363
-14.235771	-1.953637	0.660634	0.002735	0.713357
-13.963409	-1.997927	0.665638	0.002684	0.713365
-13.795086	-2.031648	0.670643	0.002652	0.713358
-14.068392	-1.992073	0.675648	0.002703	0.713340
-14.847178	-2.009673	0.680653	0.002848	0.713029
-15.180888	-1.952941	0.685658	0.002910	0.713024
-14.944475	-1.990282	0.690662	0.002866	0.713034
-14.876091	-2.006316	0.695667	0.002853	0.713026
-14.938103	-1.993358	0.700672	0.002865	0.713030
-14.698823	-2.035718	0.705677	0.002820	0.713031
-14.987277	-1.988225	0.710682	0.002874	0.713023
-15.070546	-2.074074	0.715686	0.002889	0.712823
-16.071189	-1.951481	0.720691	0.003075	0.712712
-15.613565	-2.031485	0.725696	0.002990	0.712716
-15.656497	-2.024474	0.730701	0.002998	0.712714
-15.931399	-1.978960	0.735706	0.003049	0.712708
-15.559197	-2.039711	0.740710	0.002980	0.712719
-15.975084	-1.971158	0.745715	0.003057	0.712708
-16.027263	-2.045573	0.750720	0.003067	0.712542
-16.379808	-2.060582	0.755725	0.003132	0.712387
-16.665932	-2.011500	0.760730	0.003185	0.712383
-16.910188	-1.963139	0.765734	0.003231	0.712393
-16.663250	-2.013682	0.770739	0.003185	0.712380
-16.753909	-1.993310	0.775744	0.003201	0.712389
-16.839384	-1.976879	0.780749	0.003217	0.712391
-16.836051	-2.016182	0.785754	0.003216	0.712314
-17.322725	-2.038516	0.790758	0.003307	0.712097
-17.424222	-2.023459	0.795763	0.003326	0.712091
-18.133931	-1.895467	0.800768	0.003458	0.712095
-17.477749	-2.013277	0.805773	0.003336	0.712093
-17.506929	-2.011260	0.810778	0.003341	0.712087
-17.464418	-2.013401	0.815782	0.003333	0.712098
-17.283815	-2.088027	0.820787	0.003299	0.712013
-18.390196	-2.015367	0.825792	0.003505	0.711765
-18.390443	-2.016233	0.830797	0.003505	0.711764
-18.549658	-1.990735	0.835802	0.003535	0.711758
-18.154202	-2.059789	0.840806	0.003461	0.711761
-18.593008	-1.983971	0.845811	0.003542	0.711757
-18.572173	-1.983544	0.850816	0.003538	0.711765
-18.154981	-2.098657	0.855821	0.003461	0.711684
-19.237552	-2.022233	0.860826	0.003662	0.711452
-19.263855	-2.013997	0.865830	0.003667	0.711459
-19.427457	-1.988850	0.870835	0.003697	0.711451
-19.263561	-2.015947	0.875840	0.003667	0.711456
-19.314906	-2.005988	0.880845	0.003676	0.711457
-19.646414	-1.949831	0.885850	0.003738	0.711452
-19.111543	-2.076935	0.890854	0.003638	0.711388
-20.205479	-2.008598	0.895859	0.003842	0.711136
-20.185379	-2.010273	0.900864	0.003838	0.711140
-20.272729	-1.993313	0.905869	0.003854	0.711143
-19.981838	-2.047143	0.910874	0.003800	0.711139
-20.158457	-2.013575	0.915878	0.003833	0.711144
-20.483751	-1.958053	0.920883	0.003893	0.711139
-20.231902	-2.013725	0.925888	0.003846	0.711118
-20.820686	-2.029080	0.930893	0.003956	0.710878
-21.188130	-1.967571	0.935898	0.004024	0.710870
-21.101344	-1.979135	0.940902	0.004008	0.710878
-21.043621	-1.994823	0.945907	0.003997	0.710867
-21.152629	-1.974434	0.950912	0.004017	0.710869
-20.868005	-2.021872	0.955917	0.003964	0.710876
-20.969465	-2.027607	0.960922	0.003983	0.710829
-22.006534	-1.989134	0.965926	0.004176	0.710537
-22.004237	-1.993460	0.970931	0.004175	0.710529
-21.966677	-1.996880	0.975936	0.004168	0.710536
-21.966434	-1.996348	0.980941	0.004168	0.710537
-22.373300	-1.926522	0.985946	0.004244	0.710532
-21.893497	-2.008973	0.990950	0.004154	0.710538
-21.924119	-2.006652	0.995955	0.004160	0.710532
-22.590722	-2.018147	1.000960	0.004284	0.710272
-22.839321	-1.998737	1.005965	0.004330	0.710222
-22.687784	-2.028637	1.010970	0.004302	0.710217
-22.883910	-1.989993	1.015974	0.004338	0.710224
-23.244916	-1.931186	1.020979	0.004405	0.710213
-22.770370	-2.014421	1.025984	0.004317	0.710216
-22.854796	-1.997319	1.030989	0.004333	0.710220
-23.608885	-1.967792	1.035994	0.004473	0.710011
-23.889029	-1.973975	1.040998	0.004525	0.709899
-23.457706	-2.052789	1.046003	0.004445	0.709895
-23.912895	-1.970640	1.051008	0.004529	0.709898
-24.133371	-1.928673	1.056013	0.004570	0.709903
-23.804770	-1.990941	1.061018	0.004509	0.709896
-23.835040	-1.982513	1.066022	0.004514	0.709902
-24.210268	-1.941774	1.071027	0.004584	0.709850
-24.344928	-2.044716	1.076032	0.004609	0.709596
-24.304457	-2.048973	1.081037	0.004602	0.709602
-25.149998	-1.902418	1.086042	0.004759	0.709594
-24.660544	-1.985740	1.091046	0.004668	0.709602
-24.404827	-2.035137	1.096051	0.004620	0.709595
-24.980004	-1.931842	1.101056	0.004727	0.709597
-24.599368	-2.046173	1.106061	0.004656	0.709504
-25.541897	-1.998236	1.111066	0.004831	0.709264
-25.495917	-2.001917	1.116070	0.004823	0.709273
-26.132645	-1.892369	1.121075	0.004941	0.709265
-25.663834	-1.976422	1.126080	0.004854	0.709264
-25.117496	-2.070313	1.131085	0.004752	0.709272
-25.779494	-1.957705	1.136090	0.004875	0.709261
-25.570526	-2.009495	1.141094	0.004836	0.709232
-26.087825	-2.054583	1.146099	0.004933	0.708957
-26.599718	-1.963028	1.151104	0.005028	0.708958
-26.817776	-1.921961	1.156109	0.005068	0.708963
-26.521107	-1.977212	1.161114	0.005013	0.708958
-26.467851	-1.983282	1.166118	0.005003	0.708965
-26.665076	-1.951696	1.171123	0.005039	0.708958
-26.502156	-1.979646	1.176128	0.005009	0.708961
-26.711253	-2.075779	1.181133	0.005048	0.708694
-27.684552	-1.930324	1.186138	0.005229	0.708638
-27.420941	-1.972672	1.191142	0.005180	0.708647
-26.955650	-2.059725	1.196147	0.005093	0.708639
-27.443665	-1.971098	1.201152	0.005184	0.708643
-27.395445	-1.979311	1.206157	0.005175	0.708644
-27.077536	-2.040958	1.211162	0.005116	0.708634
-27.577970	-2.091614	1.216166	0.005209	0.708354
-28.296482	-1.964638	1.221171	0.005342	0.708352
-28.548815	-1.919021	1.226176	0.005389	0.708353
-27.921128	-2.028976	1.231181	0.005272	0.708357
-28.136127	-1.995580	1.236186	0.005312	0.708348
-28.082224	-2.001380	1.241190	0.005302	0.708355
-28.054285	-2.051692	1.246195	0.005297	0.708265
-29.265493	-1.961869	1.251200	0.005522	0.708012
-28.804294	-2.041653	1.256205	0.005436	0.708017
-29.168979	-1.980879	1.261210	0.005504	0.708009
-29.054390	-1.995316	1.266214	0.005483	0.708021
-29.203602	-1.971500	1.271219	0.005510	0.708016
-29.296594	-1.953577	1.276224	0.005528	0.708019
-28.736514	-2.086242	1.281229	0.005423	0.707953
-30.075884	-1.973207	1.286234	0.005672	0.707701
-30.088590	-1.966946	1.291238	0.005675	0.707709
-30.187074	-1.952790	1.296243	0.005693	0.707702
-30.050545	-1.977170	1.301248	0.005667	0.707703
-30.029006	-1.977595	1.306253	0.005663	0.707710
-30.400094	-1.915560	1.311258	0.005732	0.707702
-29.920759	-1.997140	1.316262	0.005643	0.707709
-30.230572	-2.068931	1.321267	0.005701	0.707455
-31.219313	-1.929795	1.326272	0.005885	0.707381
-30.779777	-2.006891	1.331277	0.005803	0.707383
-30.663682	-2.032257	1.336282	0.005781	0.707374
-30.966074	-1.974140	1.341286	0.005837	0.707383
-31.023520	-1.966246	1.346291	0.005848	0.707378
-31.196677	-1.935787	1.351296	0.005880	0.707377
-31.088483	-2.036490	1.356301	0.005860	0.707214
-31.901606	-1.959223	1.361306	0.006011	0.707079
-31.401782	-2.042519	1.366310	0.005918	0.707090
-31.888798	-1.958767	1.371315	0.006008	0.707084
-32.077036	-1.925270	1.376320	0.006043	0.707084
-31.407463	-2.043287	1.381325	0.005919	0.707087
-32.020238	-1.937007	1.386330	0.006033	0.707082
-32.248113	-2.000356	1.391334	0.006075	0.706873
-32.619137	-1.994733	1.396339	0.006144	0.706752
-32.520928	-2.010421	1.401344	0.006126	0.706755
-32.525792	-2.007389	1.406349	0.006126	0.706760
-32.989485	-1.929306	1.411354	0.006213	0.706751
-32.685282	-1.978481	1.416358	0.006156	0.706761
-32.737250	-1.972959	1.421363	0.006166	0.706754
-33.162409	-1.976126	1.426368	0.006245	0.706596
-33.772550	-1.939315	1.431373	0.006358	0.706451
-33.755899	-1.947730	1.436378	0.006355	0.706440
-33.813550	-1.931330	1.441382	0.006366	0.706453
-33.432547	-2.002856	1.446387	0.006295	0.706446
-33.655075	-1.962081	1.451392	0.006336	0.706448
-33.767491	-1.941124	1.456397	0.006357	0.706450
-33.745653	-1.948366	1.461402	0.006353	0.706444
-33.883871	-2.072232	1.466406	0.006378	0.706145
-34.520108	-1.964825	1.471411	0.006497	0.706133
-34.969011	-1.885877	1.476416	0.006580	0.706131
-33.894988	-2.074901	1.481421	0.006380	0.706136
-34.333096	-2.000516	1.486426	0.006461	0.706129
-34.664525	-1.937654	1.491430	0.006523	0.706137
-34.352595	-2.017476	1.496435	0.006465	0.706088
-35.071981	-2.000867	1.501440	0.006599	0.705864
-35.213346	-1.972423	1.506445	0.006625	0.705871
-35.640008	-1.902558	1.511450	0.006704	0.705859
-35.143147	-1.984258	1.516454	0.006612	0.705873
-35.277988	-1.964348	1.521459	0.006637	0.705864
-35.780146	-1.876062	1.526464	0.006730	0.705862
-35.176727	-2.004181	1.531469	0.006618	0.705821
-36.090514	-1.990801	1.536474	0.006788	0.705520
-36.037810	-1.996289	1.541478	0.006778	0.705528
-36.240048	-1.963666	1.546483	0.006815	0.705522
-36.123722	-1.984178	1.551488	0.006794	0.705522
-36.058421	-1.992415	1.556493	0.006781	0.705529
-36.323074	-1.949172	1.561498	0.006831	0.705522
-35.866649	-2.090127	1.566502	0.006746	0.705402
-36.898066	-2.000032	1.571507	0.006938	0.705213
-37.256688	-1.935658	1.576512	0.007004	0.705214
-36.897303	-1.997399	1.581517	0.006937	0.705219
-36.913378	-1.999700	1.586522	0.006940	0.705209
-37.207620	-1.944358	1.591526	0.006995	0.705215
-37.433039	-1.903571	1.596531	0.007037	0.705216
-37.261436	-1.992029	1.601536	0.007005	0.705100
-37.679319	-2.020077	1.606541	0.007082	0.704894
-38.002368	-1.965916	1.611546	0.007142	0.704887
-38.038626	-1.955939	1.616550	0.007149	0.704894
-37.836515	-1.995616	1.621555	0.007111	0.704887
-38.117210	-1.944510	1.626560	0.007163	0.704889
-38.162160	-1.934417	1.631565	0.007172	0.704894
-37.899349	-2.029693	1.636570	0.007123	0.704796
-38.764165	-1.974817	1.641574	0.007284	0.704596
-38.699632	-1.989273	1.646579	0.007272	0.704591
-38.905029	-1.951434	1.651584	0.007310	0.704593
-38.661709	-1.994544	1.656589	0.007264	0.704594
-39.066930	-1.925772	1.661594	0.007340	0.704587
-38.674877	-1.991909	1.666598	0.007267	0.704595
-38.523474	-2.093130	1.671603	0.007238	0.704445
-40.115714	-1.901298	1.676608	0.007535	0.704260
-39.484887	-2.010155	1.681613	0.007417	0.704268
-39.521024	-2.009568	1.686618	0.007424	0.704256
-39.882971	-1.940418	1.691622	0.007491	0.704265
-39.906373	-1.938579	1.696627	0.007495	0.704261
-39.486246	-2.012936	1.701632	0.007417	0.704262
-39.561690	-2.073144	1.706637	0.007431	0.704114
-40.989680	-1.900016	1.711642	0.007697	0.703950
-40.511183	-1.981916	1.716646	0.007608	0.703957
-39.974096	-2.078748	1.721651	0.007508	0.703955
-40.592446	-1.969348	1.726656	0.007623	0.703953
-40.448040	-1.993088	1.731661	0.007596	0.703957
-40.404491	-2.005620	1.736666	0.007587	0.703948
-40.821113	-2.051927	1.741670	0.007665	0.703705
-41.538359	-1.958074	1.746675	0.007798	0.703636
-41.454122	-1.976117	1.751680	0.007783	0.703630
-41.207309	-2.016026	1.756685	0.007736	0.703639
-41.514554	-1.967145	1.761690	0.007794	0.703627
-41.322141	-1.996390	1.766694	0.007758	0.703638
-41.159933	-2.026824	1.771699	0.007727	0.703635
-42.016896	-2.005555	1.776704	0.007887	0.703369
-42.319949	-1.962598	1.781709	0.007943	0.703347
-42.286966	-1.972895	1.786714	0.007937	0.703338
-42.140012	-1.996860	1.791718	0.007909	0.703343
-42.537445	-1.926372	1.796723	0.007983	0.703343
-42.388762	-1.953892	1.801728	0.007956	0.703341
-41.892625	-2.039099	1.806733	0.007863	0.703347
-42.949219	-2.001501	1.811738	0.008060	0.703043
-43.427700	-1.932982	1.816742	0.008149	0.703009
-42.982707	-2.012977	1.821747	0.008066	0.703008
-42.940427	-2.022379	1.826752	0.008058	0.703005
-43.412832	-1.935472	1.831757	0.008146	0.703010
-43.417031	-1.940143	1.836762	0.008146	0.703000
-43.167508	-1.978802	1.841766	0.008100	0.703011
-43.243059	-2.062682	1.846771	0.008114	0.702815
-44.347869	-1.927179	1.851776	0.008319	0.702691
-44.034570	-1.980571	1.856781	0.008261	0.702696
-44.264431	-1.944277	1.861786	0.008304	0.702687
-44.229047	-1.946117	1.866790	0.008297	0.702696
-43.877798	-2.008706	1.871795	0.008232	0.702696
-44.257502	-1.942649	1.876800	0.008302	0.702693
-44.188985	-2.024834	1.881805	0.008289	0.702552
-44.826792	-2.001890	1.886810	0.008408	0.702368
-44.458223	-2.065138	1.891814	0.008339	0.702374
-45.107060	-1.950405	1.896819	0.008460	0.702372
-45.283435	-1.920401	1.901824	0.008493	0.702369
-44.470222	-2.062839	1.906829	0.008341	0.702374
-45.035800	-1.966306	1.911834	0.008446	0.702366
-45.442858	-1.989334	1.916838	0.008522	0.702173
-45.871656	-1.962283	1.921843	0.008602	0.702073
-45.795784	-1.976129	1.926848	0.008588	0.702073
-45.609387	-2.007017	1.931853	0.008553	0.702078
-45.983230	-1.943621	1.936858	0.008622	0.702071
-45.673291	-1.995261	1.941862	0.008565	0.702079
-45.650122	-2.000135	1.946867	0.008560	0.702077
-45.905490	-2.072223	1.951872	0.008608	0.701839
-46.759287	-1.963208	1.956877	0.008767	0.701752
-46.793727	-1.963634	1.961882	0.008773	0.701739
-46.547826	-2.003976	1.966886	0.008727	0.701746
-46.731928	-1.972476	1.971891	0.008761	0.701744
-46.797075	-1.960911	1.976896	0.008773	0.701744
-46.787559	-1.958995	1.981901	0.008771	0.701751
-46.992292	-2.021202	1.986906	0.008809	0.701552
-47.555748	-1.974835	1.991910	0.008914	0.701442
-47.379146	-2.007720	1.996915	0.008881	0.701440
-47.642457	-1.961052	2.001920	0.008930	0.701439

-47.493205	-1.988417	2.011917	0.008902	0.701438
-47.710553	-1.949535	2.021914	0.008942	0.701439
-48.186296	-1.971269	2.031910	0.009031	0.701223
-48.342026	-1.943487	2.041907	0.009060	0.701224
-47.959157	-2.011037	2.051904	0.008988	0.701226
-48.183357	-1.923594	2.061901	0.009030	0.701322
-47.822210	-1.932478	2.071898	0.008962	0.701435
-47.905757	-1.917489	2.081894	0.008978	0.701435
-47.680801	-1.955958	2.091891	0.008936	0.701439
-47.958441	-1.906442	2.101888	0.008987	0.701439
-47.847781	-1.927003	2.111885	0.008966	0.701438
-47.745864	-1.947164	2.121882	0.008947	0.701434
-47.788086	-1.938655	2.131878	0.008955	0.701437
-47.257467	-1.960913	2.141875	0.008856	0.701584
-46.924494	-1.941587	2.151872	0.008794	0.701743
-47.017775	-1.926137	2.161869	0.008811	0.701741
-46.896155	-1.948961	2.171866	0.008788	0.701739
-46.934857	-1.941851	2.181862	0.008795	0.701740
-46.008137	-1.960502	2.191859	0.008622	0.702037
-46.119537	-1.921698	2.201856	0.008643	0.702076
-45.635703	-2.008633	2.211853	0.008553	0.702075
-46.211433	-1.908179	2.221850	0.008660	0.702071
-45.742073	-1.902792	2.231846	0.008572	0.702251
-45.057507	-1.966005	2.241843	0.008444	0.702371
-45.368441	-1.910286	2.251840	0.008502	0.702371
-45.158246	-1.949828	2.261837	0.008463	0.702368
-44.642166	-1.885928	2.271834	0.008366	0.702683
-44.131295	-1.971262	2.281830	0.008271	0.702695
-43.950405	-2.003337	2.291827	0.008237	0.702696
-44.349877	-1.902683	2.301824	0.008312	0.702756
-43.135486	-1.995050	2.311821	0.008085	0.703007
-43.298286	-1.966823	2.321818	0.008115	0.703006
-43.427774	-1.943684	2.331814	0.008139	0.703006
-43.231713	-1.901558	2.341811	0.008103	0.703162
-42.439933	-1.952837	2.351808	0.007955	0.703344
-42.490789	-1.945108	2.361805	0.007964	0.703342
-42.522057	-1.941336	2.371802	0.007970	0.703338
-41.811912	-1.933866	2.381798	0.007837	0.703609
-41.498859	-1.976412	2.391795	0.007779	0.703637
-41.630402	-1.953333	2.401792	0.007803	0.703636
-41.517861	-1.926914	2.411789	0.007782	0.703730
-40.843847	-1.937286	2.421786	0.007657	0.703952
-40.704892	-1.962774	2.431782	0.007630	0.703951
-40.896476	-1.926824	2.441779	0.007666	0.703955
-39.845054	-1.977850	2.451776	0.007470	0.704231
-39.876299	-1.958816	2.461773	0.007476	0.704258
-39.753326	-1.981493	2.471770	0.007453	0.704257
-39.846029	-1.934336	2.481766	0.007470	0.704319
-38.902367	-1.966617	2.491763	0.007294	0.704593
-38.937809	-1.961755	2.501760	0.007300	0.704591
-38.973764	-1.954631	2.511757	0.007307	0.704593
-38.587724	-1.923881	2.521754	0.007235	0.704794
-37.889898	-2.001896	2.531750	0.007104	0.704887
-38.254407	-1.936869	2.541747	0.007172	0.704888
-37.936632	-1.961373	2.551744	0.007113	0.704953
-37.200670	-1.964725	2.561741	0.006976	0.705211
-37.076330	-1.988073	2.571738	0.006952	0.705209
-37.310862	-1.945942	2.581734	0.006996	0.705210
-36.759699	-1.941345	2.591731	0.006893	0.705417
-36.342625	-1.961623	2.601728	0.006815	0.705526
-36.275916	-1.975669	2.611725	0.006802	0.705522
-36.325681	-1.947213	2.621722	0.006812	0.705562
-35.322283	-1.977561	2.631718	0.006625	0.705861
-35.371398	-1.968129	2.641715	0.006634	0.705863
-35.343042	-1.972233	2.651712	0.006628	0.705865
-35.278715	-1.910215	2.661709	0.006616	0.706013
-34.777713	-1.943147	2.671706	0.006522	0.706127
-34.583295	-1.978634	2.681702	0.006486	0.706126
-34.773837	-1.894057	2.691699	0.006521	0.706228
-33.487497	-2.015463	2.701696	0.006282	0.706445
-33.954269	-1.932295	2.711693	0.006368	0.706446
-33.883774	-1.944141	2.721690	0.006355	0.706447
-33.184406	-1.934450	2.731686	0.006225	0.706718
-32.949378	-1.957454	2.741683	0.006181	0.706756
-32.864151	-1.973792	2.751680	0.006165	0.706754
-32.725598	-1.917980	2.761677	0.006139	0.706916
-31.952877	-1.972793	2.771674	0.005995	0.707083
-31.806620	-1.997906	2.781670	0.005967	0.707085
-32.021316	-1.958886	2.791667	0.006007	0.707087
-31.121370	-1.993723	2.801664	0.005839	0.707339
-31.294163	-1.942822	2.811661	0.005871	0.707380
-31.185092	-1.962592	2.821658	0.005851	0.707380
-31.024909	-1.929990	2.831654	0.005821	0.707503
-30.328268	-1.954107	2.841651	0.005691	0.707704
-30.388797	-1.942990	2.851648	0.005702	0.707705
-30.324690	-1.950929	2.861645	0.005690	0.707712
-29.507671	-1.947094	2.871642	0.005537	0.708012
-29.496736	-1.947660	2.881638	0.005535	0.708016
-29.535788	-1.940020	2.891635	0.005542	0.708017
-29.014457	-1.922408	2.901632	0.005445	0.708239
-28.687764	-1.924038	2.911629	0.005384	0.708353
-28.590796	-1.942000	2.921626	0.005366	0.708352
-28.673744	-1.891290	2.931622	0.005381	0.708424
-27.589774	-1.975156	2.941619	0.005179	0.708644
-27.445844	-2.000707	2.951616	0.005152	0.708644
-27.644191	-1.967216	2.961613	0.005189	0.708641
-27.151388	-1.963492	2.971610	0.005097	0.708825
-26.856356	-1.948697	2.981606	0.005042	0.708960
-26.747775	-1.966466	2.991603	0.005021	0.708964
-26.599456	-1.992564	3.001600	0.004994	0.708965
-26.289265	-1.896331	3.011597	0.004936	0.709268
-25.566218	-2.024643	3.021594	0.004801	0.709270
-25.993651	-1.948148	3.031590	0.004880	0.709271
-25.486093	-1.961219	3.041587	0.004785	0.709426
-24.845908	-1.986887	3.051584	0.004666	0.709603
-25.074733	-1.948752	3.061581	0.004709	0.709598
-24.879643	-1.984002	3.071578	0.004672	0.709598
-24.424718	-1.936391	3.081574	0.004587	0.709855
-24.153713	-1.963285	3.091571	0.004536	0.709898
-23.987916	-1.992494	3.101568	0.004505	0.709899
-24.029801	-1.926664	3.111565	0.004513	0.710016
-23.061438	-1.997783	3.121562	0.004333	0.710220
-23.440121	-1.931738	3.131558	0.004403	0.710217
-22.945074	-2.018439	3.141555	0.004311	0.710220
-22.557057	-1.955577	3.151552	0.004238	0.710485
-22.241081	-1.986080	3.161549	0.004179	0.710537
-22.171266	-1.999595	3.171546	0.004166	0.710535
-22.320876	-1.936462	3.181542	0.004194	0.710608
-21.281701	-1.986565	3.191539	0.004000	0.710878
-21.444291	-1.958673	3.201536	0.004030	0.710876
-21.443099	-1.959531	3.211533	0.004030	0.710875
-20.977410	-1.950151	3.221530	0.003943	0.711060
-20.858925	-1.929824	3.231526	0.003920	0.711143
-20.538825	-1.987226	3.241523	0.003861	0.711143
-20.751018	-1.884681	3.251520	0.003900	0.711272
-19.690921	-1.980401	3.261517	0.003702	0.711459
-19.848142	-1.953624	3.271514	0.003731	0.711456
-19.745758	-1.968594	3.281510	0.003712	0.711463
-18.954220	-1.957195	3.291507	0.003565	0.711768
-18.904509	-1.967638	3.301504	0.003555	0.711765
-18.822166	-1.984522	3.311501	0.003540	0.711761
-18.528157	-1.952465	3.321498	0.003485	0.711930
-17.987513	-1.965776	3.331494	0.003384	0.712095
-18.020656	-1.960361	3.341491	0.003390	0.712095
-18.085436	-1.943587	3.351488	0.003402	0.712106
-17.208563	-1.956025	3.361485	0.003238	0.712392
-17.036304	-1.988614	3.371482	0.003206	0.712389
-17.202631	-1.958728	3.381478	0.003237	0.712390
-16.796272	-1.941152	3.391475	0.003161	0.712569
-16.305380	-1.956859	3.401472	0.003069	0.712713
-16.254976	-1.965190	3.411469	0.003060	0.712714
-16.301802	-1.946429	3.421466	0.003068	0.712735
-15.308998	-1.977534	3.431462	0.002883	0.713026
-15.169392	-2.002304	3.441459	0.002857	0.713027
-15.475695	-1.948151	3.451456	0.002914	0.713026
-15.039127	-1.938540	3.461453	0.002833	0.713200
-14.551605	-1.943284	3.471450	0.002742	0.713364
-14.364334	-1.975956	3.481446	0.002707	0.713366
-14.422442	-1.967391	3.491443	0.002717	0.713363
-13.715987	-1.959329	3.501440	0.002585	0.713629
-13.540827	-1.978604	3.511437	0.002553	0.713653
-13.674970	-1.954100	3.521434	0.002577	0.713655
-13.489377	-1.926934	3.531430	0.002543	0.713775
-12.785532	-1.950994	3.541427	0.002411	0.713977
-12.738726	-1.959665	3.551424	0.002403	0.713977
-12.853398	-1.933793	3.561421	0.002424	0.713988
-12.132406	-1.914938	3.571418	0.002289	0.714281
-11.629400	-2.004790	3.581414	0.002195	0.714281
-11.945781	-1.947392	3.591411	0.002254	0.714283
-11.566092	-1.918983	3.601408	0.002183	0.714474
-10.926489	-1.962459	3.611405	0.002064	0.714614
-11.171232	-1.919160	3.621402	0.002109	0.714614
-10.680648	-2.004594	3.631398	0.002018	0.714618
-10.407035	-1.904571	3.641395	0.001967	0.714914
-9.853407	-2.004775	3.651392	0.001863	0.714911
-10.107480	-1.958594	3.661389	0.001911	0.714914
-9.885961	-1.923302	3.671386	0.001869	0.715062
-9.142412	-1.968763	3.681382	0.001731	0.715235
-9.320852	-1.935385	3.691379	0.001764	0.715239
-9.254545	-1.939927	3.701376	0.001751	0.715253
-8.458291	-1.930881	3.711373	0.001603	0.715553
-8.498368	-1.925850	3.721370	0.001610	0.715549
-8.274921	-1.965154	3.731366	0.001568	0.715551
-7.984811	-1.923994	3.741363	0.001514	0.715735
-6.711022	-2.074604	3.751360	0.001277	0.715887
-7.260019	-1.975740	3.761357	0.001379	0.715889
-6.874104	-2.045792	3.771354	0.001307	0.715887
-6.898973	-1.999234	3.781350	0.001311	0.715971
-6.316807	-2.019890	3.791347	0.001202	0.716136
-6.116481	-2.054522	3.801344	0.001165	0.716138
-6.248207	-2.031474	3.811341	0.001189	0.716138
-5.954320	-1.990667	3.821338	0.001134	0.716322
-5.423539	-2.019606	3.831334	0.001035	0.716453
-5.326443	-2.036680	3.841331	0.001017	0.716453
-5.179683	-2.064178	3.851328	0.000990	0.716451
-4.852428	-1.984313	3.861325	0.000928	0.716725
-4.555237	-2.019772	3.871322	0.000873	0.716760
-4.368126	-2.053271	3.881318	0.000838	0.716760
-4.280239	-2.020660	3.891315	0.000821	0.716856
-3.457708	-2.048860	3.901312	0.000668	0.717090
-3.681522	-2.011192	3.911309	0.000709	0.717086
-3.530240	-2.039692	3.921306	0.000681	0.717084
-3.225353	-1.993719	3.931302	0.000624	0.717282
-2.738034	-2.028806	3.941299	0.000533	0.717385
-2.623433	-2.048679	3.951296	0.000512	0.717386
-2.635391	-2.028392	3.961293	0.000514	0.717423
-1.766031	-2.039055	3.971290	0.000352	0.717708
-1.738397	-2.042176	3.981286	0.000346	0.717712
-1.795189	-2.032317	3.991283	0.000357	0.717712
-1.639891	-1.985786	4.001280	0.000328	0.717859
-1.531460	-1.923023	4.011277	0.000307	0.718021
-1.441030	-1.939777	4.021274	0.000290	0.718020
-1.720428	-1.793415	4.031270	0.000342	0.718212
-1.011750	-1.843988	4.041267	0.000210	0.718361
-1.060838	-1.832970	4.051264	0.000219	0.718366
-0.824283	-1.732565	4.061261	0.000175	0.718648
-0.863863	-1.726405	4.071258	0.000182	0.718647
-1.043666	-1.584470	4.081254	0.000215	0.718864
-0.947615	-1.548967	4.091251	0.000197	0.718968
-0.687155	-1.482130	4.101248	0.000148	0.719192
-0.786628	-1.421374	4.111245	0.000166	0.719277
-0.609481	-1.304935	4.121242	0.000133	0.719569
-0.456132	-1.290522	4.131238	0.000104	0.719652
-0.193747	-1.208491	4.141235	0.000055	0.719906
-0.450914	-1.083566	4.151232	0.000103	0.720062
-0.189933	-1.044811	4.161229	0.000054	0.720231
-0.055632	-0.918638	4.171226	0.000029	0.720527
-0.086750	-0.825437	4.181222	0.000034	0.720700
-0.327447	-0.676041	4.191219	0.000079	0.720910
-0.345927	-0.562604	4.201216	0.000082	0.721127
0.007223	-0.489113	4.211213	0.000016	0.721395
0.011488	-0.377344	4.221210	0.000015	0.721617
0.093997	-0.262812	4.231206	-0.000001	0.721871
0.307813	-0.166399	4.241203	-0.000041	0.722136
0.470569	-0.070633	4.251200	-0.000071	0.722381
0.321079	0.116426	4.261197	-0.000044	0.722697
0.000000	0.342630	4.271194	0.000016	0.723029

-0.004966	0.973576	4.276198	0.000016	0.724264
0.462758	2.143341	4.281203	-0.000072	0.726715
0.839977	3.928440	4.286208	-0.000143	0.730323
1.289707	6.265643	4.291213	-0.000229	0.735004
1.440102	9.154833	4.296218	-0.000259	0.740611
1.760610	12.498316	4.301222	-0.000320	0.747097
2.221683	16.272935	4.306227	-0.000409	0.754386
2.549093	20.473230	4.311232	-0.000473	0.762353
3.194214	25.027724	4.316237	-0.000596	0.770993
3.621210	29.979067	4.321242	-0.000679	0.780189
4.013461	35.296340	4.326246	-0.000755	0.789923
4.305530	40.940987	4.331251	-0.000813	0.800089
4.837096	46.842483	4.336256	-0.000916	0.810650
5.272896	53.051138	4.341261	-0.001002	0.821577
5.548606	59.555097	4.346266	-0.001057	0.832815
6.186455	66.213366	4.351270	-0.001180	0.844270
6.581099	73.143807	4.356275	-0.001259	0.855951
6.889752	80.282490	4.361280	-0.001321	0.867791
7.352686	87.592872	4.366285	-0.001412	0.879792
9.952742	94.699227	4.371290	-0.001901	0.891903
12.911084	101.972763	4.376294	-0.002456	0.904212
13.431846	109.832651	4.381299	-0.002559	0.916600
14.217530	117.749190	4.386304	-0.002710	0.928979
15.157290	125.776216	4.391309	-0.002890	0.941403
15.863402	133.931592	4.396314	-0.003027	0.953794
17.132354	142.068916	4.401318	-0.003269	0.966143
18.426205	150.295856	4.406323	-0.003515	0.978472
19.080765	158.715972	4.411328	-0.003643	0.990764
19.811962	167.176485	4.416333	-0.003785	1.002981
20.629890	175.649896	4.421338	-0.003942	1.015090
21.434340	184.162907	4.426342	-0.004098	1.027107
22.365716	192.704525	4.431347	-0.004277	1.039053
23.112663	201.292859	4.436352	-0.004422	1.050883
23.931898	209.897065	4.441357	-0.004580	1.062619
24.631216	218.553646	4.446362	-0.004716	1.074267
25.536646	227.157977	4.451366	-0.004890	1.085769
26.098689	235.852557	4.456371	-0.005001	1.097190
26.765807	244.507264	4.461376	-0.005131	1.108465
27.904715	253.105496	4.466381	-0.005348	1.119657
28.931657	261.723390	4.471386	-0.005545	1.130738
29.701889	270.379805	4.476390	-0.005694	1.141704
30.053587	279.129233	4.481395	-0.005766	1.152592
30.656250	287.778262	4.486400	-0.005884	1.163308
31.612542	296.364560	4.491405	-0.006067	1.173923
32.143353	305.001429	4.496410	-0.006172	1.184415
32.944338	313.597836	4.501414	-0.006327	1.194822
34.028748	322.125590	4.506419	-0.006534	1.205115
34.270323	330.794207	4.511424	-0.006585	1.215317
35.146304	339.338335	4.516429	-0.006754	1.225415
36.083818	347.884353	4.521434	-0.006934	1.235444
36.849862	356.403749	4.526438	-0.007082	1.245328
37.331764	364.987137	4.531443	-0.007178	1.255152
38.076047	373.480386	4.536448	-0.007322	1.264848
38.573408	382.043734	4.541453	-0.007420	1.274502
39.206462	390.527881	4.546458	-0.007544	1.284021
39.755113	399.036788	4.551462	-0.007652	1.293481
40.652157	407.481038	4.556467	-0.007824	1.302865
41.327632	416.025049	4.561472	-0.007956	1.312249
41.973120	424.512286	4.566477	-0.008081	1.321500
42.574271	432.925077	4.571482	-0.008199	1.330600
43.063150	441.349210	4.576486	-0.008296	1.339629
43.625121	449.763031	4.581491	-0.008406	1.348600
44.075395	458.177215	4.586496	-0.008495	1.357492
44.926640	466.504776	4.591501	-0.008659	1.366305
45.210337	474.939783	4.596506	-0.008718	1.375075
45.424851	483.363707	4.601510	-0.008763	1.383766
46.425535	491.672278	4.606515	-0.008955	1.392419
46.983962	500.016317	4.611520	-0.009064	1.400979
47.436646	508.386793	4.616525	-0.009154	1.409495
48.219978	516.685282	4.621530	-0.009306	1.417944
48.740973	525.014765	4.626534	-0.009408	1.426329
49.249152	533.377243	4.631539	-0.009508	1.434696
49.813381	541.671066	4.636544	-0.009619	1.442956
50.487833	549.973409	4.641549	-0.009750	1.451194
50.911552	558.295667	4.646554	-0.009834	1.459365
51.151099	566.646455	4.651558	-0.009885	1.467489
51.843716	574.977828	4.656563	-0.010019	1.475621
52.392053	583.223836	4.661568	-0.010127	1.483603
52.757090	591.533176	4.666573	-0.010200	1.491575
53.259815	599.806402	4.671578	-0.010299	1.499491
54.005924	608.035403	4.676582	-0.010444	1.507361
54.425437	616.334732	4.681587	-0.010527	1.515205
54.994351	624.565289	4.686592	-0.010639	1.522968
55.713945	632.797454	4.691597	-0.010778	1.530716
56.172917	641.066594	4.696602	-0.010869	1.538419
56.540178	649.326577	4.701606	-0.010943	1.546062
56.927617	657.625199	4.706611	-0.011020	1.553705
57.449378	665.826537	4.711616	-0.011123	1.561242
57.891024	674.072828	4.716621	-0.011211	1.568771
58.759343	682.244175	4.721626	-0.011378	1.576259
59.252406	690.471028	4.726630	-0.011475	1.583707
59.774353	698.715595	4.731635	-0.011578	1.591139
60.054147	706.970982	4.736640	-0.011635	1.598512
60.711120	715.155708	4.741645	-0.011763	1.605842
60.923916	723.431304	4.746650	-0.011808	1.613156
61.326507	731.637432	4.751654	-0.011889	1.620402
62.291110	739.780241	4.756659	-0.012074	1.627639
62.334130	748.105874	4.761664	-0.012087	1.634875
62.795314	756.291105	4.766669	-0.012178	1.642015
63.301344	764.466857	4.771674	-0.012278	1.649122
63.714644	772.663658	4.776678	-0.012360	1.656204
63.982209	780.884722	4.781683	-0.012416	1.663257
64.497277	789.045444	4.786688	-0.012517	1.670261
65.165145	797.229210	4.791693	-0.012647	1.677276
65.552207	805.401649	4.796698	-0.012724	1.684215
65.847623	813.612661	4.801702	-0.012785	1.691146
66.186709	821.820881	4.806707	-0.012853	1.698051
66.705601	829.965246	4.811712	-0.012955	1.704899
67.188463	838.160306	4.816717	-0.013051	1.711756
67.636029	846.336550	4.821722	-0.013139	1.718566
68.200655	854.460987	4.826726	-0.013250	1.725322
68.691561	862.633067	4.831731	-0.013347	1.732080
68.722787	870.853425	4.836736	-0.013358	1.738793
69.358093	878.961719	4.841741	-0.013482	1.745465
69.627949	887.169989	4.846746	-0.013537	1.752147
70.138954	895.310835	4.851750	-0.013638	1.758779
70.768574	903.421475	4.856755	-0.013761	1.765376
71.337323	911.574537	4.861760	-0.013872	1.771975
71.899930	919.727392	4.866765	-0.013982	1.778549
72.283141	927.884723	4.871770	-0.014059	1.785080
72.708755	936.086896	4.876774	-0.014144	1.791627
73.137512	944.283357	4.881779	-0.014229	1.798146
73.192637	952.432496	4.886784	-0.014244	1.804559
73.665283	960.565422	4.891789	-0.014338	1.810987
74.124156	968.707614	4.896794	-0.014429	1.817398
74.553179	976.822500	4.901798	-0.014514	1.823761
74.983011	984.964627	4.906803	-0.014599	1.830123
75.548594	993.083093	4.911808	-0.014710	1.836461
76.165020	1001.188846	4.916813	-0.014830	1.842773
76.657893	1009.332338	4.921818	-0.014927	1.849078
77.173170	1017.474912	4.926822	-0.015029	1.855363
77.815431	1025.587002	4.931827	-0.015154	1.861618
78.159345	1033.748008	4.936832	-0.015223	1.867855
78.672339	1041.913765	4.941837	-0.015324	1.874094
78.965195	1050.047856	4.946842	-0.015384	1.880263
79.372699	1058.165949	4.951846	-0.015465	1.886412
79.641159	1066.342671	4.956851	-0.015521	1.892570
80.062216	1074.446964	4.961856	-0.015604	1.898671
80.418524	1082.577236	4.966861	-0.015676	1.904764
80.797132	1090.706075	4.971866	-0.015752	1.910839
81.409939	1098.797888	4.976870	-0.015872	1.916894
81.703226	1106.939853	4.981875	-0.015932	1.922930
81.864213	1115.081244	4.986880	-0.015967	1.928933
82.385737	1123.196077	4.991885	-0.016069	1.934937
82.971594	1131.279851	4.996890	-0.016184	1.940907
83.198109	1139.423403	5.001894	-0.016231	1.946863
83.287848	1147.640159	5.006899	-0.016254	1.952839
83.600915	1155.729343	5.011904	-0.016317	1.958728
84.363293	1163.763695	5.016909	-0.016465	1.964608
84.639098	1171.883426	5.021914	-0.016521	1.970480
84.906011	1180.013922	5.026918	-0.016576	1.976341
85.369596	1188.108283	5.031923	-0.016668	1.982180
85.806303	1196.202418	5.036928	-0.016755	1.987999
86.252452	1204.326947	5.041933	-0.016843	1.993823
86.437307	1212.449519	5.046938	-0.016883	1.999601
86.614372	1220.555560	5.051942	-0.016921	2.005349
87.013707	1228.668591	5.056947	-0.017001	2.011110
87.423378	1236.758559	5.061952	-0.017083	2.016839
88.071922	1244.823293	5.066957	-0.017209	2.022558
88.441451	1252.933911	5.071962	-0.017283	2.028264
88.914731	1261.058049	5.076966	-0.017377	2.033975
89.349544	1269.154161	5.081971	-0.017463	2.039645
89.588314	1277.254549	5.086976	-0.017513	2.045283
89.970622	1285.370283	5.091981	-0.017589	2.050931
90.545836	1293.446716	5.096986	-0.017702	2.056555
90.830245	1301.550216	5.101990	-0.017760	2.062154
91.193690	1309.666283	5.106995	-0.017833	2.067753
91.639832	1317.774324	5.112000	-0.017922	2.073340
92.153415	1325.857886	5.117005	-0.018023	2.078902
92.395491	1333.951220	5.122010	-0.018073	2.084429
92.685855	1342.050479	5.127014	-0.018132	2.089949
93.112876	1350.168714	5.132019	-0.018217	2.095482
93.422026	1358.235659	5.137024	-0.018280	2.100953
93.959668	1366.309480	5.142029	-0.018386	2.106437
94.241760	1374.461199	5.147034	-0.018444	2.111935
94.401236	1382.592732	5.152038	-0.018479	2.117392
94.794178	1390.649526	5.157043	-0.018557	2.122808
94.990262	1398.726144	5.162048	-0.018599	2.128205
95.509773	1406.811400	5.167053	-0.018701	2.133624
95.977560	1414.876904	5.172058	-0.018794	2.139012
96.047908	1422.982350	5.177062	-0.018812	2.144374
96.444123	1431.069675	5.182067	-0.018891	2.149742
96.715633	1439.164889	5.187072	-0.018947	2.155090
97.007874	1447.257461	5.192077	-0.019007	2.160425
97.468145	1455.314360	5.197082	-0.019098	2.165739
98.020332	1463.364222	5.202086	-0.019206	2.171044
98.353703	1471.487323	5.207091	-0.019274	2.176363
98.692323	1479.551363	5.212096	-0.019342	2.181631
99.183837	1487.626803	5.217101	-0.019439	2.186908
99.525047	1495.744566	5.222106	-0.019508	2.192186
99.882400	1503.823402	5.227110	-0.019580	2.197427
100.505042	1511.870830	5.232115	-0.019701	2.202659
100.876831	1519.927114	5.237120	-0.019776	2.207862
101.120531	1528.055834	5.242125	-0.019826	2.213088
101.377824	1536.146502	5.247130	-0.019880	2.218278
101.559707	1544.221747	5.252134	-0.019919	2.223439
101.880032	1552.318422	5.257139	-0.019984	2.228614
102.254358	1560.390641	5.262144	-0.020059	2.233767
102.692080	1568.460344	5.267149	-0.020146	2.238911
103.080537	1576.516928	5.272154	-0.020223	2.244031
103.586045	1584.581632	5.277158	-0.020323	2.249155
104.141764	1592.666337	5.282163	-0.020432	2.254283
104.280412	1600.756904	5.287168	-0.020463	2.259368
104.501684	1608.856366	5.292173	-0.020509	2.264453
105.374636	1616.874582	5.297178	-0.020677	2.269533
105.579902	1625.054278	5.302182	-0.020721	2.274644
105.784374	1633.120088	5.307187	-0.020764	2.279673
105.859806	1641.178525	5.312192	-0.020784	2.284675
106.091607	1649.261991	5.317197	-0.020832	2.289695
106.419835	1657.334943	5.322202	-0.020899	2.294706
106.750570	1665.369109	5.327206	-0.020966	2.299682
107.217878	1673.423582	5.332211	-0.021058	2.304671
107.339333	1681.514069	5.337216	-0.021086	2.309642
107.767047	1689.595094	5.342221	-0.021171	2.314623
108.167861	1697.629675	5.347226	-0.021251	2.319562
108.288121	1705.704205	5.352230	-0.021279	2.324491
108.473931	1713.811995	5.357235	-0.021319	2.329436
108.776641	1721.870287	5.362240	-0.021380	2.334349
109.296344	1729.923084	5.367245	-0.021483	2.339267
109.843673	1737.964883	5.372250	-0.021590	2.344170
110.302841	1746.026482	5.377254	-0.021681	2.349067
110.540222	1754.153074	5.382259	-0.021730	2.353976
110.777463	1762.199728	5.387264	-0.021780	2.358825
111.010237	1770.267367	5.392269	-0.021828	2.363678
111.384017	1778.325233	5.397274	-0.021903	2.368525
111.724513	1786.384952	5.402278	-0.021972	2.373361
112.022492	1794.473867	5.407283	-0.022033	2.378201
112.514906	1802.486676	5.412288	-0.022130	2.383001
112.974361	1810.548577	5.417293	-0.022221	2.387819
113.441231	1818.625031	5.422298	-0.022313	2.392635
113.689405	1826.691901	5.427302	-0.022365	2.397419
114.139931	1834.767512	5.432307	-0.022454	2.402214
114.605215	1842.806874	5.437312	-0.022546	2.406980
115.036314	1850.878995	5.442317	-0.022632	2.411752
115.288316	1858.971101	5.447322	-0.022684	2.416513
115.692439	1867.018356	5.452326	-0.022764	2.421250
116.241749	1875.078017	5.457331	-0.022872	2.425996
116.445373	1883.182206	5.462336	-0.022915	2.430731
116.596864	1891.349522	5.467341	-0.022949	2.435491
117.013553	1899.365587	5.472346	-0.023032	2.440173
117.247307	1907.375989	5.477350	-0.023081	2.444830
117.756639	1915.424130	5.482355	-0.023181	2.449520
118.059921	1923.479766	5.487360	-0.023243	2.454189
118.245042	1931.548467	5.492365	-0.023282	2.458849
118.576072	1939.591830	5.497370	-0.023349	2.463496
118.974935	1947.618889	5.502374	-0.023429	2.468130
119.297248	1955.727473	5.507379	-0.023494	2.472796
119.331353	1963.795199	5.512384	-0.023506	2.477408
119.615910	1971.833760	5.517389	-0.023564	2.482014
120.116810	1979.854788	5.522394	-0.023663	2.486617
120.577285	1987.913552	5.527398	-0.023754	2.491230
120.831588	1996.006986	5.532403	-0.023807	2.495839
120.971963	2004.052945	5.537408	-0.023838	2.500404
121.645136	2012.060956	5.542413	-0.023969	2.504978
121.910267	2020.152217	5.547418	-0.024024	2.509561
122.160914	2028.268629	5.552422	-0.024076	2.514148
122.513104	2036.318087	5.557427	-0.024147	2.518697
122.646915	2044.353416	5.562432	-0.024177	2.523214
122.792025	2052.416304	5.567437	-0.024209	2.527740
123.117159	2060.482546	5.572442	-0.024275	2.532271
123.284629	2068.534502	5.577446	-0.024312	2.536776
123.639468	2076.586903	5.582451	-0.024383	2.541286
123.869622	2084.618784	5.587456	-0.024431	2.545767
124.047343	2092.709897	5.592461	-0.024470	2.550270
123.991260	2100.818758	5.597466	-0.024465	2.554758
124.507330	2108.801834	5.602470	-0.024566	2.559209
124.912496	2116.835467	5.607475	-0.024647	2.563673
124.953837	2124.893984	5.612480	-0.024660	2.568116
125.392823	2132.939540	5.617485	-0.024747	2.572573
125.797549	2141.001633	5.622490	-0.024828	2.577028
126.030026	2149.054765	5.627494	-0.024876	2.581459
126.398973	2157.099396	5.632499	-0.024950	2.585887
126.824265	2165.146441	5.637504	-0.025035	2.590313
127.885999	2173.322702	5.642509	-0.025238	2.594844
128.284100	2181.320440	5.647514	-0.025317	2.599225
128.706601	2189.322567	5.652518	-0.025401	2.603603
129.055345	2197.376080	5.657523	-0.025472	2.607996
129.270768	2205.417796	5.662528	-0.025517	2.612367
129.674048	2213.484846	5.667533	-0.025598	2.616756
129.840635	2221.527197	5.672538	-0.025634	2.621109
129.908036	2229.572931	5.677542	-0.025652	2.625450
130.241390	2237.626014	5.682547	-0.025719	2.629805
130.542124	2245.679795	5.687552	-0.025780	2.634151
130.897079	2253.706622	5.692557	-0.025852	2.638479
131.107862	2261.767716	5.697562	-0.025897	2.642809
131.280331	2269.798622	5.702566	-0.025934	2.647113
131.839567	2277.847899	5.707571	-0.026043	2.651445
132.040749	2285.912388	5.712576	-0.026086	2.655755
132.140795	2293.968928	5.717581	-0.026110	2.660046
132.474267	2302.003129	5.722586	-0.026178	2.664335
132.829488	2310.043715	5.727590	-0.026249	2.668620
133.146261	2318.144603	5.732595	-0.026313	2.672929
133.244943	2326.194073	5.737600	-0.026337	2.677189
133.611208	2334.208146	5.742605	-0.026411	2.681441
133.926011	2342.246702	5.747610	-0.026475	2.685696
134.042468	2350.285228	5.752614	-0.026502	2.689931
134.415011	2358.361673	5.757619	-0.026576	2.694196
134.765664	2366.390000	5.762624	-0.026647	2.698427
135.049401	2374.427214	5.767629	-0.026705	2.702652
135.462261	2382.455769	5.772634	-0.026787	2.706874
135.559750	2390.531741	5.777638	-0.026811	2.711094
135.974385	2398.595779	5.782643	-0.026893	2.715321
136.076956	2406.623253	5.787648	-0.026918	2.719503
136.392893	2414.652257	5.792653	-0.026982	2.723693
136.618844	2422.721350	5.797658	-0.027029	2.727892
136.858925	2430.768758	5.802662	-0.027079	2.732073
137.393307	2438.812005	5.807667	-0.027184	2.736264
137.532060	2446.846163	5.812672	-0.027215	2.740420
137.578718	2454.890112	5.817677	-0.027229	2.744569
137.896367	2462.969054	5.822682	-0.027294	2.748746
138.304277	2471.034683	5.827686	-0.027375	2.752915
138.613233	2479.104887	5.832691	-0.027438	2.757074
138.797211	2487.125844	5.837696	-0.027478	2.761194
139.250973	2495.118843	5.842701	-0.027567	2.765310
139.394500	2503.185257	5.847706	-0.027600	2.769438
139.673931	2511.225317	5.852710	-0.027657	2.773555
140.023955	2519.272358	5.857715	-0.027727	2.777674
140.255047	2527.294341	5.862720	-0.027776	2.781766
140.493933	2535.335374	5.867725	-0.027826	2.785863
140.861709	2543.374106	5.872730	-0.027899	2.789960
141.180223	2551.423148	5.877734	-0.027964	2.794053
141.402322	2559.484779	5.882739	-0.028011	2.798141
141.628165	2567.509621	5.887744	-0.028058	2.802205
142.059387	2575.523911	5.892749	-0.028144	2.806269
142.381164	2583.576268	5.897754	-0.028209	2.810340
142.515189	2591.651398	5.902758	-0.028239	2.814406
142.847491	2599.694479	5.907763	-0.028307	2.818461
143.172959	2607.706471	5.912768	-0.028372	2.822495
143.267523	2615.768253	5.917773	-0.028395	2.826534
143.657447	2623.811826	5.922778	-0.028473	2.830575
144.182349	2631.864962	5.927782	-0.028576	2.834623
144.224113	2639.918760	5.932787	-0.028590	2.838638
144.338174	2647.938144	5.937792	-0.028616	2.842634
144.686102	2655.962622	5.942797	-0.028686	2.846640
145.084896	2664.001693	5.947802	-0.028766	2.850650
145.497522	2672.026164	5.952806	-0.028848	2.854649
145.670154	2680.092844	5.957811	-0.028885	2.858649
145.893080	2688.109006	5.962816	-0.028932	2.862621
146.229444	2696.147813	5.967821	-0.029000	2.866606
146.555657	2704.220059	5.972826	-0.029066	2.870600
146.879699	2712.261429	5.977830	-0.029132	2.874574
147.031752	2720.328156	5.982835	-0.029166	2.878545
147.100224	2728.348527	5.987840	-0.029184	2.882484
147.375356	2736.378050	5.992845	-0.029240	2.886432
147.710753	2744.408865	5.997850	-0.029308	2.890379
147.879855	2752.488400	6.002854	-0.029345	2.894336
148.310208	2760.508025	6.007859	-0.029430	2.898272
148.533869	2768.549999	6.012864	-0.029477	2.902202
148.951918	2776.563029	6.017869	-0.029560	2.906123
149.209505	2784.620143	6.022874	-0.029614	2.910052
149.432669	2792.744212	6.027878	-0.029661	2.914006
149.564733	2800.792049	6.032883	-0.029691	2.917913
149.931724	2808.748305	6.037888	-0.029764	2.921783
150.270892	2816.753250	6.042893	-0.029833	2.925669
150.489065	2824.791241	6.047898	-0.029879	2.929560
150.742190	2832.862178	6.052902	-0.029931	2.933464
151.033126	2840.900974	6.057907	-0.029991	2.937348
151.812501	2848.876987	6.062912	-0.030141	2.941223
151.831308	2856.932986	6.067917	-0.030150	2.945092
152.235151	2864.962690	6.072922	-0.030230	2.948962
152.373490	2873.018007	6.077926	-0.030262	2.952826
152.785869	2881.075460	6.082931	-0.030344	2.956700
152.910209	2889.081010	6.087936	-0.030372	2.960530
153.373290	2897.105984	6.092941	-0.030464	2.964381
153.621736	2905.173733	6.097946	-0.030515	2.968236
153.760412	2913.215205	6.102950	-0.030546	2.972068
153.924928	2921.291351	6.107955	-0.030582	2.975914
154.355687	2929.284599	6.112960	-0.030668	2.979728
154.665333	2937.311041	6.117965	-0.030731	2.983547
154.902653	2945.372750	6.122970	-0.030780	2.987373
154.986290	2953.416860	6.127974	-0.030801	2.991180
155.471470	2961.475302	6.132979	-0.030897	2.995007
155.488203	2969.487537	6.137984	-0.030905	2.998785
155.827691	2977.494603	6.142989	-0.030974	3.002572
156.257148	2985.523134	6.147994	-0.031059	3.006368
156.479805	2993.545084	6.152998	-0.031106	3.010147
156.932412	3001.617185	6.158003	-0.031196	3.013955
157.183843	3009.640665	6.163008	-0.031248	3.017726
157.292170	3017.692535	6.168013	-0.031273	3.021498
157.572409	3025.722655	6.173018	-0.031331	3.025264
157.816947	3033.750566	6.178022	-0.031382	3.029022
158.068740	3041.820004	6.183027	-0.031434	3.032795
158.089602	3049.883862	6.188032	-0.031443	3.036550
158.402490	3057.859787	6.193037	-0.031507	3.040273
158.895211	3065.885705	6.198042	-0.031604	3.044024
159.023298	3073.932245	6.203046	-0.031633	3.047762
159.318951	3081.985745	6.208051	-0.031693	3.051506
159.651238	3090.044206	6.213056	-0.031761	3.055250
159.987116	3098.038673	6.218061	-0.031828	3.058960
160.111612	3106.092972	6.223066	-0.031857	3.062683
160.273256	3114.114062	6.228070	-0.031892	3.066388
160.710878	3122.141389	6.233075	-0.031979	3.070104
160.722365	3130.286339	6.238080	-0.031987	3.073850
161.176613	3138.278845	6.243085	-0.032077	3.077542
161.684792	3146.278478	6.248090	-0.032177	3.081235
161.752545	3154.257283	6.253094	-0.032194	3.084893
161.932380	3162.316949	6.258099	-0.032233	3.088590
162.158242	3170.347584	6.263104	-0.032281	3.092271
162.290284	3178.435615	6.268109	-0.032311	3.095969
162.509337	3186.454141	6.273114	-0.032357	3.099635
162.820638	3194.445652	6.278118	-0.032420	3.103289
163.194410	3202.481742	6.283123	-0.032495	3.106961
163.093589	3210.543003	6.288128	-0.032481	3.110619
163.327534	3218.592259	6.293133	-0.032530	3.114283
163.735045	3226.607088	6.298138	-0.032612	3.117934
163.812124	3234.649630	6.303142	-0.032631	3.121578
164.095823	3242.634303	6.308147	-0.032689	3.125202
164.347836	3250.670929	6.313152	-0.032742	3.128843
164.555223	3258.755356	6.318157	-0.032786	3.132499
164.873993	3266.802396	6.323162	-0.032850	3.136140
165.135540	3274.772236	6.328166	-0.032904	3.139738
165.486422	3282.810052	6.333171	-0.032975	3.143367
165.750431	3290.840052	6.338176	-0.033029	3.146985
165.786263	3298.915509	6.343181	-0.033041	3.150609
166.284996	3306.968000	6.348186	-0.033140	3.154238
166.494657	3314.986769	6.353190	-0.033184	3.157835
166.963721	3322.960416	6.358195	-0.033277	3.161420
167.214112	3330.966508	6.363200	-0.033329	3.165005
167.475328	3339.012291	6.368205	-0.033383	3.168604
167.650475	3347.090341	6.373210	-0.033420	3.172210
167.878619	3355.097487	6.378214	-0.033468	3.175783
168.226900	3363.137442	6.383219	-0.033538	3.179371
168.470347	3371.155136	6.388224	-0.033589	3.182941
168.496835	3379.198365	6.393229	-0.033599	3.186509
168.914106	3387.250217	6.398234	-0.033682	3.190093
169.103248	3395.263047	6.403238	-0.033723	3.193646
169.390862	3403.322953	6.408243	-0.033782	3.197220
169.566054	3411.331871	6.413248	-0.033820	3.200763
169.782210	3419.317565	6.418253	-0.033865	3.204293
170.178044	3427.382536	6.423258	-0.033944	3.207862
170.421194	3435.417754	6.428262	-0.033995	3.211407
170.852779	3443.470655	6.433267	-0.034081	3.214964
171.105883	3451.483890	6.438272	-0.034133	3.218492
171.064603	3459.536315	6.443277	-0.034131	3.222022
171.440029	3467.533872	6.448282	-0.034206	3.225540
171.740529	3475.568720	6.453286	-0.034267	3.229068
171.960141	3483.652158	6.458291	-0.034314	3.232610
172.100678	3491.723261	6.463296	-0.034345	3.236139
172.456544	3499.676686	6.468301	-0.034417	3.239622
172.711932	3507.681076	6.473306	-0.034469	3.243120
172.661193	3515.718736	6.478310	-0.034465	3.246615
172.928346	3523.752465	6.483315	-0.034520	3.250118
173.182531	3531.786113	6.488320	-0.034573	3.253617
173.334619	3539.824165	6.493325	-0.034607	3.257109
173.618729	3547.837290	6.498330	-0.034665	3.260592
174.001963	3555.823429	6.503334	-0.034742	3.264064
174.246198	3563.896600	6.508339	-0.034792	3.267564
174.484744	3571.926272	6.513344	-0.034842	3.271041
174.602375	3579.973344	6.518349	-0.034869	3.274518
174.974217	3587.980790	6.523354	-0.034944	3.277983
175.083055	3596.013982	6.528358	-0.034970	3.281446
175.434153	3604.008594	6.533363	-0.035040	3.284898
175.559208	3612.053086	6.538368	-0.035069	3.288358
175.704473	3620.113052	6.543373	-0.035101	3.291823
175.996256	3628.153246	6.548378	-0.035161	3.295281
176.116707	3636.177133	6.553382	-0.035189	3.298721
176.330372	3644.223108	6.558387	-0.035234	3.302172
176.622041	3652.217354	6.563392	-0.035293	3.305599
176.824692	3660.243996	6.568397	-0.035336	3.309033
177.004153	3668.331663	6.573402	-0.035375	3.312489
177.154428	3676.360043	6.578406	-0.035408	3.315915
177.573161	3684.338785	6.583411	-0.035492	3.319326
177.905346	3692.343796	6.588416	-0.035559	3.322741
178.100143	3700.369196	6.593421	-0.035601	3.326157
178.414143	3708.397725	6.598426	-0.035664	3.329574
178.576364	3716.444894	6.603430	-0.035700	3.332991
178.746930	3724.525506	6.608435	-0.035737	3.336418
178.935774	3732.496244	6.613440	-0.035777	3.339796
179.048011	3740.527593	6.618445	-0.035804	3.343193
179.574685	3748.564815	6.623450	-0.035907	3.346605
179.592042	3756.586068	6.628454	-0.035916	3.349988
179.869968	3764.648002	6.633459	-0.035973	3.353393
179.913543	3772.730877	6.638464	-0.035986	3.356796
180.394521	3780.646473	6.643469	-0.036081	3.360141
180.416076	3788.699277	6.648474	-0.036090	3.363523
180.717508	3796.718582	6.653478	-0.036152	3.366898
180.872020	3804.763741	6.658483	-0.036186	3.370275
181.139481	3812.840338	6.663488	-0.036241	3.373666
181.300608	3820.844537	6.668493	-0.036276	3.377019
181.726579	3828.854692	6.673498	-0.036361	3.380381
182.008837	3836.876854	6.678502	-0.036419	3.383739
182.263217	3844.895978	6.683507	-0.036472	3.387092
182.362869	3852.952590	6.688512	-0.036495	3.390452
182.455517	3861.049357	6.693517	-0.036518	3.393824
182.855973	3869.077561	6.698522	-0.036598	3.397176
183.050982	3876.997053	6.703526	-0.036639	3.400472
183.474997	3885.023578	6.708531	-0.036724	3.403816
183.478526	3893.065772	6.713536	-0.036730	3.407150
183.773644	3901.062433	6.718541	-0.036790	3.410472
184.113104	3909.129839	6.723546	-0.036859	3.413821
184.068461	3917.158955	6.728550	-0.036856	3.417137
184.421524	3925.142174	6.733555	-0.036927	3.420446
184.689566	3933.180361	6.738560	-0.036982	3.423770
184.776687	3941.205584	6.743565	-0.037003	3.427080
185.024435	3949.248343	6.748570	-0.037055	3.430399
185.356084	3957.290707	6.753574	-0.037122	3.433718
185.458676	3965.338224	6.758579	-0.037146	3.437028
185.669963	3973.345230	6.763584	-0.037191	3.440322
185.867248	3981.336768	6.768589	-0.037233	3.443605
186.244856	3989.384860	6.773594	-0.037309	3.446915
186.375372	3997.407208	6.778598	-0.037338	3.450203
186.612323	4005.469273	6.783603	-0.037388	3.453507
186.735000	4013.530684	6.788608	-0.037416	3.456804
186.991853	4021.505785	6.793613	-0.037469	3.460067
187.013926	4029.545433	6.798618	-0.037479	3.463346
187.245770	4037.566183	6.803622	-0.037527	3.466621
187.721995	4045.574613	6.808627	-0.037621	3.469895
188.118073	4053.648610	6.813632	-0.037700	3.473191
188.556916	4061.656369	6.818637	-0.037787	3.476457
189.149230	4069.641400	6.823642	-0.037903	3.479716
188.982840	4077.648681	6.828646	-0.037877	3.482957
189.373678	4085.711774	6.833651	-0.037955	3.486235
189.702608	4093.714891	6.838656	-0.038022	3.489484
189.718034	4101.741391	6.843661	-0.038030	3.492729
189.946520	4109.823111	6.848666	-0.038078	3.496000
190.239828	4117.790637	6.853670	-0.038138	3.499225
190.597247	4125.828137	6.858675	-0.038210	3.502476
190.687050	4133.861985	6.863680	-0.038232	3.505714
190.691439	4141.871802	6.868685	-0.038238	3.508937
191.202186	4149.904786	6.873690	-0.038338	3.512182
191.305905	4157.937502	6.878694	-0.038363	3.515412
191.451433	4165.955808	6.883699	-0.038395	3.518634
191.596751	4173.993240	6.888704	-0.038428	3.521860
191.776262	4181.973153	6.893709	-0.038466	3.525062
191.960546	4190.030299	6.898714	-0.038506	3.528292
192.188998	4198.069731	6.903718	-0.038554	3.531513
192.567286	4206.095236	6.908723	-0.038630	3.534730
192.490152	4214.133269	6.913728	-0.038621	3.537935
192.477691	4222.166698	6.918733	-0.038624	3.541137
193.199630	4230.152870	6.923738	-0.038763	3.544340
193.393316	4238.214765	6.928742	-0.038805	3.547554
193.440052	4246.228933	6.933747	-0.038819	3.550742
193.517885	4254.381708	6.938752	-0.038839	3.553983
193.919384	4262.340332	6.943757	-0.038919	3.557153
194.022800	4270.350930	6.948762	-0.038943	3.560333
193.949614	4278.342228	6.953766	-0.038935	3.563497
194.371451	4286.351082	6.958771	-0.039019	3.566679
194.787934	4294.351093	6.963776	-0.039102	3.569855
195.013721	4302.392011	6.968781	-0.039149	3.573038
195.247519	4310.453083	6.973786	-0.039198	3.576227
195.504408	4318.406553	6.978790	-0.039251	3.579371
195.576440	4326.465242	6.983795	-0.039270	3.582549
195.872363	4334.486513	6.988800	-0.039330	3.585715
196.025778	4342.497415	6.993805	-0.039364	3.588870
196.440788	4350.551630	6.998810	-0.039447	3.592047
196.619525	4358.550426	7.003814	-0.039485	3.595193
196.818993	4366.565992	7.008819	-0.039528	3.598343
197.159527	4374.596237	7.013824	-0.039597	3.601500
197.168357	4382.564562	7.018829	-0.039603	3.604621
197.618488	4390.629310	7.023834	-0.039693	3.607789
197.836698	4398.623342	7.028838	-0.039739	3.610920
198.036269	4406.706490	7.033843	-0.039781	3.614082
198.143122	4414.745654	7.038848	-0.039806	3.617223
198.350925	4422.722357	7.043853	-0.039850	3.620338
198.685652	4430.768589	7.048858	-0.039918	3.623482
198.685246	4438.789769	7.053862	-0.039923	3.626604
199.025925	4446.804793	7.058867	-0.039992	3.629730
199.400546	4454.863944	7.063872	-0.040067	3.632871
199.578277	4462.910758	7.068877	-0.040105	3.636000
199.838630	4470.911433	7.073882	-0.040159	3.639110
200.078596	4478.901930	7.078886	-0.040209	3.642213
200.069362	4486.922744	7.083891	-0.040213	3.645318
200.381430	4494.949620	7.088896	-0.040276	3.648432
200.494103	4502.991316	7.093901	-0.040303	3.651543
200.984973	4511.059740	7.098906	-0.040399	3.654672
200.950321	4519.041101	7.103910	-0.040398	3.657751
201.399824	4527.060749	7.108915	-0.040487	3.660855
201.614420	4535.099045	7.113920	-0.040532	3.663957
201.733401	4543.131149	7.118925	-0.040560	3.667051
202.078219	4551.153481	7.123930	-0.040629	3.670145
202.378740	4559.152349	7.128934	-0.040691	3.673226
202.573709	4567.191888	7.133939	-0.040732	3.676318
202.621404	4575.201567	7.138944	-0.040747	3.679391
202.909648	4583.201377	7.143949	-0.040806	3.682465
203.060367	4591.263491	7.148954	-0.040839	3.685556
203.282302	4599.267399	7.153958	-0.040886	3.688624
203.578617	4607.288764	7.158963	-0.040946	3.691698
203.819602	4615.340165	7.163968	-0.040996	3.694779
204.015048	4623.314599	7.168973	-0.041038	3.697827
204.317888	4631.380522	7.173978	-0.041100	3.700911
204.393882	4639.366237	7.178982	-0.041119	3.703955
204.412844	4647.411439	7.183987	-0.041128	3.707019
204.766110	4655.415698	7.188992	-0.041199	3.710072
204.821454	4663.530316	7.193997	-0.041215	3.713157
205.109661	4671.589241	7.199002	-0.041274	3.716225
205.390809	4679.513005	7.204006	-0.041331	3.719238
205.380061	4687.521043	7.209011	-0.041335	3.722274
205.725225	4695.500885	7.214016	-0.041404	3.725305
205.838366	4703.520902	7.219021	-0.041431	3.728343
206.175359	4711.589695	7.224026	-0.041499	3.731403
206.283775	4719.605113	7.229030	-0.041524	3.734434
206.611350	4727.639967	7.234035	-0.041591	3.737476
206.729208	4735.652272	7.239040	-0.041618	3.740501
206.925087	4743.626542	7.244045	-0.041660	3.743512
207.279202	4751.698762	7.249050	-0.041731	3.746561
207.273809	4759.715101	7.254054	-0.041735	3.749577
207.507105	4767.769834	7.259059	-0.041784	3.752612
207.850993	4775.811165	7.264064	-0.041853	3.755641
208.282749	4783.773951	7.269069	-0.041939	3.758640
208.513316	4791.848715	7.274074	-0.041987	3.761675
208.315616	4799.815941	7.279078	-0.041956	3.764656
208.809456	4807.862926	7.284083	-0.042053	3.767681
209.074840	4815.911927	7.289088	-0.042108	3.770699
209.352009	4823.898305	7.294093	-0.042165	3.773692
209.430914	4831.973169	7.299098	-0.042185	3.776710
209.405490	4839.952800	7.304102	-0.042185	3.779689
209.779390	4847.967027	7.309107	-0.042260	3.782687
209.999338	4856.006908	7.314112	-0.042307	3.785688
210.033618	4864.017215	7.319117	-0.042318	3.788672
210.394634	4872.093630	7.324122	-0.042391	3.791685
210.614354	4880.120201	7.329126	-0.042437	3.794675
211.013313	4888.126815	7.334131	-0.042517	3.797658
210.979202	4896.129662	7.339136	-0.042516	3.800628
211.069316	4904.097069	7.344141	-0.042538	3.803586
211.390634	4912.138310	7.349146	-0.042603	3.806573
211.406128	4920.130190	7.354150	-0.042611	3.809534
211.489400	4928.188565	7.359155	-0.042632	3.812518
212.163456	4936.213739	7.364160	-0.042763	3.815499
212.225055	4944.221930	7.369165	-0.042779	3.818460
212.314103	4952.261888	7.374170	-0.042801	3.821430
212.432701	4960.249760	7.379174	-0.042829	3.824379
212.798355	4968.296066	7.384179	-0.042902	3.827353
213.192651	4976.332780	7.389184	-0.042981	3.830321
213.312294	4984.321643	7.394189	-0.043009	3.833264
213.614993	4992.390606	7.399194	-0.043070	3.836238
213.708781	5000.363652	7.404198	-0.043093	3.839170
214.090749	5008.382223	7.409203	-0.043169	3.842122
214.416264	5016.369382	7.414208	-0.043235	3.845059
214.768598	5024.403921	7.419213	-0.043306	3.848012
214.823277	5032.472978	7.424218	-0.043322	3.850969
214.958007	5040.485043	7.429222	-0.043352	3.853905
215.091255	5048.569110	7.434227	-0.043382	3.856864
215.212218	5056.555013	7.439232	-0.043410	3.859786
215.493221	5064.542689	7.444237	-0.043468	3.862708
215.886867	5072.555324	7.449242	-0.043546	3.865640
216.020853	5080.585520	7.454246	-0.043577	3.868571
216.173465	5088.631166	7.459251	-0.043610	3.871506
216.301764	5096.901297	7.464256	-0.043640	3.874520
216.540034	5104.845056	7.469261	-0.043689	3.877414
216.720832	5112.756650	7.474266	-0.043728	3.880294
216.821840	5120.717936	7.479270	-0.043752	3.883188
217.125510	5128.733991	7.484275	-0.043814	3.886104
217.498026	5136.750901	7.489280	-0.043889	3.889019
217.527159	5144.760775	7.494285	-0.043900	3.891923
217.869420	5152.836364	7.499290	-0.043969	3.894854
217.890601	5160.827703	7.504294	-0.043978	3.897746
218.060038	5168.819122	7.509299	-0.044015	3.900640
218.154601	5176.885198	7.514304	-0.044038	3.903556
218.453078	5184.880386	7.519309	-0.044099	3.906449
218.771543	5192.883219	7.524314	-0.044163	3.909342
218.703552	5200.917692	7.529318	-0.044156	3.912238
219.045402	5208.960898	7.534323	-0.044225	3.915142
219.262582	5216.986979	7.539328	-0.044271	3.918035
219.280548	5224.938743	7.544333	-0.044279	3.920896
219.587833	5232.954934	7.549338	-0.044342	3.923784
219.786226	5240.966907	7.554342	-0.044384	3.926665
219.876481	5249.013680	7.559347	-0.044406	3.929555
220.072359	5257.062979	7.564352	-0.044448	3.932446
220.364888	5265.036016	7.569357	-0.044508	3.935309
220.806362	5273.081859	7.574362	-0.044595	3.938198
220.855913	5281.103948	7.579366	-0.044610	3.941070
221.099279	5289.088497	7.584371	-0.044661	3.943930
221.408194	5297.140469	7.589376	-0.044723	3.946813
221.308265	5305.145468	7.594381	-0.044710	3.949670
221.975230	5313.190528	7.599386	-0.044840	3.952552
221.901094	5321.228796	7.604390	-0.044831	3.955417
221.904222	5329.235905	7.609395	-0.044837	3.958270
222.242801	5337.255798	7.614400	-0.044905	3.961131
222.485727	5345.208888	7.619405	-0.044956	3.963965
222.739015	5353.277973	7.624410	-0.045008	3.966838
222.870173	5361.247949	7.629414	-0.045038	3.969672
223.147320	5369.326876	7.634419	-0.045095	3.972545
223.331500	5377.350045	7.639424	-0.045135	3.975395
223.325616	5385.356955	7.644429	-0.045139	3.978233
223.685891	5393.375759	7.649434	-0.045211	3.981080
224.098704	5401.383954	7.654438	-0.045294	3.983921
224.356093	5409.419226	7.659443	-0.045347	3.986768
224.470140	5417.450044	7.664448	-0.045373	3.989609
224.449069	5425.506863	7.669453	-0.045375	3.992455
224.716172	5433.566261	7.674458	-0.045430	3.995304
224.842380	5441.558128	7.679462	-0.045459	3.998125
225.216446	5449.543817	7.684467	-0.045534	4.000945
225.584636	5457.569259	7.689472	-0.045607	4.003778
225.564645	5465.557285	7.694477	-0.045609	4.006589
225.571989	5473.617204	7.699482	-0.045616	4.009424
225.800439	5481.664317	7.704486	-0.045664	4.012256
225.988841	5489.678945	7.709491	-0.045704	4.015074
226.194701	5497.705655	7.714496	-0.045748	4.017895
226.291736	5505.664420	7.719501	-0.045771	4.020688
226.709700	5513.697900	7.724506	-0.045854	4.023510
226.831436	5521.680273	7.729510	-0.045882	4.026307
226.897070	5529.717929	7.734515	-0.045900	4.029122
227.201157	5537.802071	7.739520	-0.045962	4.031953
227.309758	5545.884163	7.744525	-0.045987	4.034780
227.679900	5553.905599	7.749530	-0.046062	4.037587
227.848963	5561.816768	7.754534	-0.046098	4.040350
228.032433	5569.803575	7.759539	-0.046138	4.043139
228.112404	5577.824441	7.764544	-0.046158	4.045935
228.260368	5585.835554	7.769549	-0.046191	4.048728
228.627125	5593.896275	7.774554	-0.046264	4.051538
228.664271	5601.907008	7.779558	-0.046277	4.054325
228.899340	5609.926954	7.784563	-0.046326	4.057116
228.910724	5617.925563	7.789568	-0.046333	4.059894
229.151655	5625.909672	7.794573	-0.046383	4.062669
229.452838	5633.940166	7.799578	-0.046445	4.065458
229.415724	5642.014956	7.804582	-0.046443	4.068256
229.807638	5649.983692	7.809587	-0.046521	4.071022
230.344122	5658.055205	7.814592	-0.046627	4.073823
230.493513	5666.062753	7.819597	-0.046660	4.076595
230.899192	5674.013454	7.824602	-0.046741	4.079348
230.935307	5682.064467	7.829606	-0.046753	4.082130
231.091593	5690.055749	7.834611	-0.046787	4.084890
231.512291	5698.086753	7.839616	-0.046871	4.087666
231.526102	5706.102654	7.844621	-0.046879	4.090429
231.740759	5714.176217	7.849626	-0.046924	4.093213
232.075426	5722.168292	7.854630	-0.046992	4.095969
232.254323	5730.188986	7.859635	-0.047030	4.098730
232.465254	5738.263943	7.864640	-0.047075	4.101509
232.471016	5746.192081	7.869645	-0.047081	4.104232
232.764105	5754.259536	7.874650	-0.047141	4.107005
233.019161	5762.250220	7.879654	-0.047194	4.109750
232.975031	5770.338356	7.884659	-0.047191	4.112522
233.353421	5778.383781	7.889664	-0.047267	4.115283
233.482236	5786.334327	7.894669	-0.047296	4.118007
233.800543	5794.360064	7.899674	-0.047361	4.120757
234.146390	5802.369311	7.904678	-0.047430	4.123500
234.373313	5810.366331	7.909683	-0.047478	4.126235
234.543432	5818.417412	7.914688	-0.047515	4.128986
234.743090	5826.419819	7.919693	-0.047557	4.131719
235.017685	5834.516584	7.924698	-0.047614	4.134483
235.034306	5842.530704	7.929702	-0.047622	4.137214
235.038992	5850.474429	7.934707	-0.047628	4.139920
235.549806	5858.544546	7.939712	-0.047729	4.142672
235.514567	5866.517682	7.944717	-0.047728	4.145383
235.594405	5874.569311	7.949722	-0.047748	4.148120
235.774383	5882.587978	7.954726	-0.047787	4.150846
236.041870	5890.642185	7.959731	-0.047842	4.153583
236.204997	5898.685049	7.964736	-0.047878	4.156313
236.586681	5906.620072	7.969741	-0.047954	4.159007
236.794416	5914.664789	7.974746	-0.047998	4.161734
237.030117	5922.646613	7.979750	-0.048047	4.164438
237.060536	5930.700425	7.984755	-0.048058	4.167163
237.336520	5938.692455	7.989760	-0.048115	4.169868
237.434760	5946.733417	7.994765	-0.048138	4.172586
237.804912	5954.774672	7.999770	-0.048213	4.175305
237.861878	5962.759089	8.004774	-0.048229	4.178000
238.217995	5970.760543	8.009779	-0.048300	4.180701
238.366618	5978.815549	8.014784	-0.048333	4.183417
238.550672	5986.755116	8.019789	-0.048373	4.186093
238.707665	5994.828751	8.024794	-0.048407	4.188811
238.834794	6002.826905	8.029798	-0.048436	4.191503
238.921913	6010.991311	8.034803	-0.048458	4.194247
239.143176	6019.011046	8.039808	-0.048504	4.196943
239.219313	6026.899927	8.044813	-0.048524	4.199592
239.255260	6034.961685	8.049818	-0.048536	4.202297
239.531947	6042.857514	8.054822	-0.048593	4.204946
239.828138	6050.936851	8.059827	-0.048653	4.207656
240.009352	6058.924165	8.064832	-0.048692	4.210332
239.987894	6066.949638	8.069837	-0.048694	4.213017
240.445897	6075.041027	8.074842	-0.048784	4.215726
240.655442	6083.017876	8.079846	-0.048828	4.218394
240.556204	6091.027418	8.084851	-0.048815	4.221068
240.881132	6099.040231	8.089856	-0.048881	4.223745
241.120037	6107.004515	8.094861	-0.048931	4.226403
241.279915	6115.062341	8.099866	-0.048966	4.229090
241.266227	6123.075819	8.104870	-0.048969	4.231759
241.587860	6131.124487	8.109875	-0.049034	4.234441
241.819146	6139.192146	8.114880	-0.049082	4.237127
241.823433	6147.100245	8.119885	-0.049088	4.239756
242.135735	6155.179760	8.124890	-0.049152	4.242443
242.218993	6163.182274	8.129894	-0.049173	4.245101
242.255597	6171.183561	8.134899	-0.049185	4.247756
242.575279	6179.280325	8.139904	-0.049250	4.250444
242.794173	6187.236106	8.144909	-0.049296	4.253082
243.025278	6195.303161	8.149914	-0.049344	4.255756
242.993028	6203.268040	8.154918	-0.049343	4.258392
243.329601	6211.336948	8.159923	-0.049411	4.261064
243.523701	6219.303218	8.164928	-0.049453	4.263699
243.609345	6227.357602	8.169933	-0.049474	4.266360
243.782762	6235.349584	8.174938	-0.049512	4.269000
243.939796	6243.426509	8.179942	-0.049546	4.271666
244.286095	6251.441364	8.184947	-0.049616	4.274312
244.479507	6259.491618	8.189952	-0.049658	4.276966
244.544174	6267.423967	8.194957	-0.049675	4.279579
244.904736	6275.487852	8.199962	-0.049747	4.282236
245.061602	6283.410806	8.204966	-0.049782	4.284843
245.341866	6291.497240	8.209971	-0.049839	4.287503
245.655631	6299.488210	8.214976	-0.049903	4.290131
245.669853	6307.529256	8.219981	-0.049911	4.292771
246.041323	6315.583179	8.224986	-0.049986	4.295416
246.131562	6323.582009	8.229990	-0.050008	4.298040
246.111580	6331.582559	8.234995	-0.050009	4.300661
246.122637	6339.644507	8.240000	-0.050017	4.303301
246.532199	6347.578463	8.245005	-0.050098	4.305901
246.641304	6355.629073	8.250010	-0.050124	4.308535
246.751641	6363.656928	8.255014	-0.050150	4.311160
247.016417	6371.715046	8.260019	-0.050204	4.313794
247.171562	6379.740395	8.265024	-0.050239	4.316416
247.161341	6387.706271	8.270029	-0.050242	4.319015
247.317713	6395.740461	8.275034	-0.050276	4.321636
247.615574	6403.701883	8.280038	-0.050337	4.324232
247.753205	6411.746342	8.285043	-0.050368	4.326853
247.791480	6419.793950	8.290048	-0.050381	4.329473
248.005663	6427.792945	8.295053	-0.050426	4.332076
248.410951	6435.817964	8.300058	-0.050507	4.334688
248.501257	6443.880247	8.305062	-0.050529	4.337308
248.667411	6451.814181	8.310067	-0.050565	4.339885
249.012300	6459.835052	8.315072	-0.050634	4.342490
249.178669	6467.842204	8.320077	-0.050671	4.345088
249.373157	6475.884516	8.325082	-0.050712	4.347696
249.614318	6483.885542	8.330086	-0.050762	4.350289
249.630892	6492.010474	8.335091	-0.050771	4.352919
249.771788	6500.072380	8.340096	-0.050803	4.355528
249.860583	6507.974982	8.345101	-0.050824	4.358084
250.037084	6515.961846	8.350106	-0.050862	4.360666
250.128734	6523.991800	8.355110	-0.050885	4.363259
250.252981	6531.960199	8.360115	-0.050913	4.365832
250.518023	6540.009294	8.365120	-0.050968	4.368430
250.576430	6548.008774	8.370125	-0.050984	4.371009
250.921449	6556.074950	8.375130	-0.051054	4.373610
251.258018	6564.085114	8.380134	-0.051122	4.376191
251.542254	6572.032127	8.385139	-0.051180	4.378749
251.915241	6580.094106	8.390144	-0.051255	4.381344
252.062670	6588.063683	8.395149	-0.051287	4.383906
252.458849	6596.108805	8.400154	-0.051367	4.386492
252.689140	6604.108976	8.405158	-0.051415	4.389062
252.760367	6612.180704	8.410163	-0.051433	4.391652
253.141471	6620.296206	8.415168	-0.051510	4.394256
253.294047	6628.232132	8.420173	-0.051543	4.396800
253.449235	6636.185359	8.425178	-0.051578	4.399348
253.630648	6644.243367	8.430182	-0.051617	4.401928
253.792820	6652.192246	8.435187	-0.051652	4.404471
253.967244	6660.270648	8.440192	-0.051690	4.407055
254.154704	6668.240300	8.445197	-0.051730	4.409602
254.251813	6676.304930	8.450202	-0.051754	4.412178
254.626589	6684.349856	8.455206	-0.051829	4.414747
254.682509	6692.356081	8.460211	-0.051844	4.417300
254.872532	6700.364152	8.465216	-0.051885	4.419854
255.039564	6708.384111	8.470221	-0.051922	4.422410
255.288944	6716.387089	8.475226	-0.051973	4.424959
255.545067	6724.417275	8.480230	-0.052026	4.427515
255.798301	6732.426717	8.485235	-0.052079	4.430063
255.542649	6740.514169	8.490240	-0.052037	4.432633
255.675259	6748.548266	8.495245	-0.052067	4.435185
256.056347	6756.533820	8.500250	-0.052143	4.437722
256.100681	6764.481929	8.505254	-0.052156	4.440244
256.220149	6772.513456	8.510259	-0.052184	4.442791
256.397378	6780.501670	8.515264	-0.052222	4.445323
256.659892	6788.569453	8.520269	-0.052276	4.447880
257.056323	6796.595090	8.525274	-0.052356	4.450421
257.129868	6804.655734	8.530278	-0.052375	4.452972
257.421401	6812.628770	8.535283	-0.052434	4.455494
257.597617	6820.681806	8.540288	-0.052472	4.458039
257.736002	6828.600499	8.545293	-0.052503	4.460540
258.016242	6836.648870	8.550298	-0.052561	4.463082
258.149689	6844.660873	8.555302	-0.052591	4.465610
258.257616	6852.673769	8.560307	-0.052616	4.468136
258.618724	6860.731393	8.565312	-0.052689	4.470676
258.700625	6868.739902	8.570317	-0.052710	4.473199
258.903493	6876.745883	8.575322	-0.052753	4.475719
259.008704	6884.786153	8.580327	-0.052778	4.478248
259.212554	6892.758612	8.585331	-0.052821	4.480755
259.359653	6900.799733	8.590336	-0.052854	4.483282
259.389295	6908.768899	8.595341	-0.052864	4.485785
259.719091	6916.835535	8.600346	-0.052931	4.488318
259.892307	6924.847421	8.605351	-0.052969	4.490831
259.980361	6932.864553	8.610355	-0.052990	4.493345
260.187858	6940.880301	8.615360	-0.053034	4.495857
260.249967	6948.899735	8.620365	-0.053051	4.498368
260.501170	6956.883364	8.625370	-0.053103	4.500867
260.832184	6964.923877	8.630375	-0.053170	4.503383
260.988730	6972.878346	8.635379	-0.053205	4.505870
261.177095	6980.970999	8.640384	-0.053245	4.508399
261.270705	6988.934894	8.645389	-0.053268	4.510886
261.640902	6997.030534	8.650394	-0.053342	4.513413
261.885745	7005.057559	8.655399	-0.053393	4.515917
261.908267	7013.017357	8.660403	-0.053403	4.518398
262.318385	7021.017370	8.665408	-0.053484	4.520892
262.264010	7029.008547	8.670413	-0.053479	4.523380
262.452283	7037.007804	8.675418	-0.053520	4.525870
262.692480	7045.074529	8.680423	-0.053570	4.528379
263.012170	7053.041958	8.685427	-0.053635	4.530856
263.201958	7061.132115	8.690432	-0.053675	4.533370
263.440422	7069.072747	8.695437	-0.053725	4.535836
263.739327	7077.140294	8.700442	-0.053786	4.538340
264.017181	7085.174256	8.705447	-0.053843	4.540833
264.006843	7093.121244	8.710451	-0.053846	4.543296
264.273405	7101.132959	8.715456	-0.053901	4.545779
264.274852	7109.156194	8.720461	-0.053907	4.548263
264.380829	7117.209694	8.725466	-0.053932	4.550756
264.621314	7125.291449	8.730471	-0.053982	4.553256
264.813824	7133.262740	8.735475	-0.054023	4.555721
265.005666	7141.267743	8.740480	-0.054064	4.558194
264.949063	7149.266725	8.745485	-0.054059	4.560664
265.113507	7157.277570	8.750490	-0.054095	4.563137
265.331523	7165.274487	8.755495	-0.054141	4.565604
265.375732	7173.310629	8.760499	-0.054154	4.568082
265.802269	7181.357522	8.765504	-0.054239	4.570561
266.004164	7189.387039	8.770509	-0.054282	4.573034
266.259923	7197.446273	8.775514	-0.054335	4.575515
266.335308	7205.407699	8.780519	-0.054354	4.577964
266.417144	7213.344980	8.785523	-0.054375	4.580405
266.672115	7221.434742	8.790528	-0.054428	4.582891
266.501402	7229.445941	8.795533	-0.054401	4.585351
266.847211	7237.510956	8.800538	-0.054471	4.587827
267.132864	7245.517384	8.805543	-0.054530	4.590283
267.093409	7253.504842	8.810547	-0.054527	4.592733
267.236423	7261.567896	8.815552	-0.054559	4.595204
267.411740	7269.548701	8.820557	-0.054597	4.597648
267.653009	7277.511419	8.825562	-0.054648	4.600086
267.791479	7285.570252	8.830567	-0.054679	4.602552
267.801180	7293.488356	8.835571	-0.054686	4.604973
268.078537	7301.619345	8.840576	-0.054743	4.607458
268.278896	7309.586072	8.845581	-0.054785	4.609892
268.412188	7317.634733	8.850586	-0.054816	4.612349
268.638440	7325.643893	8.855591	-0.054863	4.614793
268.685047	7333.683690	8.860595	-0.054877	4.617245
268.939613	7341.664690	8.865600	-0.054930	4.619678
269.006083	7349.695713	8.870605	-0.054947	4.622124
269.311842	7357.653660	8.875610	-0.055010	4.624547
269.315276	7365.715678	8.880615	-0.055016	4.627001
269.544718	7373.718966	8.885619	-0.055064	4.629435
269.910359	7381.776279	8.890624	-0.055137	4.631884
269.778395	7389.757280	8.895629	-0.055118	4.634310
269.870587	7397.782253	8.900634	-0.055140	4.636747
270.012325	7405.805498	8.905639	-0.055172	4.639182
270.232185	7413.792142	8.910643	-0.055218	4.641604
270.433865	7421.800489	8.915648	-0.055261	4.644032
270.628830	7429.833695	8.920653	-0.055303	4.646467
270.969329	7437.843998	8.925658	-0.055371	4.648892
271.153430	7445.859973	8.930663	-0.055411	4.651319
271.221418	7453.883789	8.935667	-0.055429	4.653747
271.551206	7461.945142	8.940672	-0.055496	4.656184
271.582380	7469.918393	8.945677	-0.055507	4.658594
271.728800	7477.943961	8.950682	-0.055539	4.661018
272.072381	7485.971766	8.955687	-0.055609	4.663441
272.167264	7493.953822	8.960691	-0.055632	4.665850
272.215054	7501.992570	8.965696	-0.055646	4.668274
272.198480	7509.999907	8.970701	-0.055648	4.670688
272.568616	7518.060482	8.975706	-0.055722	4.673116
272.849443	7526.150742	8.980711	-0.055780	4.675552
272.910031	7534.080963	8.985715	-0.055797	4.677939
273.124358	7542.046435	8.990720	-0.055842	4.680335
273.427714	7550.069682	8.995725	-0.055904	4.682747
273.560202	7558.026318	9.000730	-0.055934	4.685137
273.564044	7566.121267	9.005735	-0.055940	4.687569
273.781257	7574.055642	9.010739	-0.055985	4.689950
273.983053	7582.120991	9.015744	-0.056028	4.692370
273.841829	7590.164898	9.020749	-0.056007	4.694782
274.056344	7598.181472	9.025754	-0.056053	4.697185
274.361708	7606.147769	9.030759	-0.056115	4.699571
274.581151	7614.156080	9.035763	-0.056161	4.701968
274.829839	7622.184483	9.040768	-0.056213	4.704370
274.962742	7630.164886	9.045773	-0.056243	4.706757
274.981659	7638.219368	9.050778	-0.056251	4.709165
275.158357	7646.292025	9.055783	-0.056290	4.711577
275.202926	7654.277695	9.060787	-0.056303	4.713962
275.533772	7662.328847	9.065792	-0.056370	4.716364
275.520463	7670.286571	9.070797	-0.056373	4.718738
275.884551	7678.271033	9.075802	-0.056446	4.721118
275.899648	7686.331456	9.080807	-0.056454	4.723521
275.952714	7694.352374	9.085811	-0.056469	4.725910
276.277952	7702.381385	9.090816	-0.056535	4.728299
276.287465	7710.375423	9.095821	-0.056542	4.730678
276.538224	7718.441304	9.100826	-0.056594	4.733077
276.577249	7726.401815	9.105831	-0.056607	4.735443
276.684176	7734.460656	9.110835	-0.056632	4.737837
276.977852	7742.428048	9.115840	-0.056692	4.740203
277.066627	7750.455985	9.120845	-0.056714	4.742585
277.167786	7758.471313	9.125850	-0.056738	4.744963
277.460847	7766.539431	9.130855	-0.056798	4.747355
277.571288	7774.485106	9.135859	-0.056824	4.749709
277.896187	7782.558751	9.140864	-0.056890	4.752100
277.951159	7790.596166	9.145869	-0.056905	4.754479
278.202471	7798.608577	9.150874	-0.056957	4.756849
278.271232	7806.554017	9.155879	-0.056976	4.759199
278.366549	7814.644263	9.160883	-0.056999	4.761591
278.462195	7822.557914	9.165888	-0.057022	4.763929
278.634358	7830.586530	9.170893	-0.057059	4.766299
278.963363	7838.617213	9.175898	-0.057126	4.768669
279.064210	7846.631806	9.180903	-0.057150	4.771033
279.016289	7854.650368	9.185907	-0.057146	4.773398
279.314731	7862.678020	9.190912	-0.057207	4.775763
279.549444	7870.702460	9.195917	-0.057256	4.778126
279.667863	7878.659211	9.200922	-0.057283	4.780468
279.953877	7886.764675	9.205927	-0.057342	4.782853
280.109742	7894.636607	9.210931	-0.057376	4.785168
280.381012	7902.777636	9.215936	-0.057432	4.787560
280.462624	7910.704109	9.220941	-0.057453	4.789889
280.656524	7918.802145	9.225946	-0.057494	4.792267
280.851292	7926.831970	9.230951	-0.057536	4.794623
280.890334	7934.847286	9.235955	-0.057548	4.796975
281.092038	7942.826697	9.240960	-0.057591	4.799314
281.268484	7950.806461	9.245965	-0.057629	4.801653
281.488292	7958.822908	9.250970	-0.057676	4.804000
281.721842	7966.872399	9.255975	-0.057724	4.806357
281.793909	7974.838824	9.260979	-0.057743	4.808688
281.915583	7982.913565	9.265984	-0.057771	4.811050
281.811107	7990.376385	9.270989	-0.057757	4.813233
281.996561	7995.116310	9.275994	-0.057794	4.814617

282.406925	7997.708892	9.280999	-0.057873	4.815373
282.337339	7999.073028	9.286003	-0.057861	4.815772
282.707902	7999.578725	9.291008	-0.057930	4.815918
282.712196	8000.500923	9.296013	-0.057931	4.816187
282.815672	8000.503882	9.301018	-0.057951	4.816187
282.861354	8000.461980	9.306023	-0.057959	4.816175
283.002541	8000.506228	9.311027	-0.057986	4.816187
283.181104	8000.418659	9.316032	-0.058019	4.816161
282.912310	8000.538799	9.321037	-0.057969	4.816197
283.315888	8000.556831	9.326042	-0.058044	4.816200
283.214614	8000.502641	9.331047	-0.058026	4.816185
283.090242	8000.453373	9.336051	-0.058003	4.816171
283.226060	8000.549882	9.341056	-0.058028	4.816199
283.327499	8000.520748	9.346061	-0.058047	4.816190
283.164880	8000.448346	9.351066	-0.058017	4.816169
283.446609	8000.413941	9.356071	-0.058069	4.816158
283.495124	8000.475739	9.361075	-0.058078	4.816176
283.633700	8000.472925	9.366080	-0.058104	4.816174
283.378865	8000.527070	9.371085	-0.058057	4.816191
283.632410	8000.461166	9.376090	-0.058104	4.816171
283.824206	8000.574723	9.381095	-0.058140	4.816203
283.736083	8000.543210	9.386099	-0.058124	4.816194
283.831041	8000.487244	9.391104	-0.058142	4.816177
283.923391	8000.487864	9.396109	-0.058159	4.816177
284.032225	8000.441768	9.401114	-0.058179	4.816163
283.835020	8000.498029	9.406119	-0.058143	4.816180
283.882075	8000.505305	9.411123	-0.058151	4.816182
284.030601	8000.264386	9.416128	-0.058179	4.816111
283.930937	8000.573531	9.421133	-0.058161	4.816202
283.909545	8000.496215	9.426138	-0.058157	4.816179
284.194862	8000.439437	9.431143	-0.058210	4.816161
283.914808	8000.520905	9.436147	-0.058158	4.816187
284.176148	8000.503228	9.441152	-0.058207	4.816180
284.028593	8000.558255	9.446157	-0.058179	4.816197
284.234318	8000.464767	9.451162	-0.058218	4.816168
284.142988	8000.533640	9.456167	-0.058201	4.816189
284.259281	8000.587056	9.461171	-0.058223	4.816204
284.295319	8000.493686	9.466176	-0.058229	4.816177
284.192541	8000.442672	9.471181	-0.058210	4.816162
284.225664	8000.583265	9.476186	-0.058217	4.816203
284.500918	8000.512413	9.481191	-0.058268	4.816181
284.372942	8000.489792	9.486195	-0.058244	4.816175
284.373806	8000.513325	9.491200	-0.058244	4.816182
284.499152	8000.532711	9.496205	-0.058268	4.816187
284.689096	8000.576782	9.501210	-0.058303	4.816199
284.543347	8000.564522	9.506215	-0.058276	4.816196
284.442818	8000.469736	9.511219	-0.058258	4.816169
284.643139	8000.378287	9.516224	-0.058295	4.816141
284.566857	8000.571388	9.521229	-0.058281	4.816198
284.615630	8000.514581	9.526234	-0.058290	4.816181
284.788837	8000.310438	9.531239	-0.058322	4.816120
284.696258	8000.429512	9.536243	-0.058305	4.816156
284.867919	8000.285181	9.541248	-0.058337	4.816113
284.549839	8000.497392	9.546253	-0.058278	4.816176
284.829861	8000.471506	9.551258	-0.058330	4.816167
284.772673	8000.479024	9.556263	-0.058320	4.816170
284.781436	8000.475986	9.561267	-0.058322	4.816169
284.959591	8000.557243	9.566272	-0.058355	4.816192
284.820863	8000.477790	9.571277	-0.058329	4.816169
284.815762	8000.506558	9.576282	-0.058328	4.816178
284.901663	8000.590411	9.581287	-0.058344	4.816202
284.761835	8000.563298	9.586291	-0.058318	4.816194
284.654147	8000.500439	9.591296	-0.058298	4.816177
284.611311	8000.501806	9.596301	-0.058291	4.816177
284.630347	8000.520327	9.601306	-0.058294	4.816182
284.821372	8000.509920	9.606311	-0.058330	4.816178
284.688812	8000.434854	9.611315	-0.058305	4.816157
284.926759	8000.439192	9.616320	-0.058350	4.816157
285.035489	8000.535214	9.621325	-0.058370	4.816185
284.952904	8000.448234	9.626330	-0.058355	4.816160
284.896131	8000.426907	9.631335	-0.058344	4.816154
284.898039	8000.511369	9.636339	-0.058345	4.816178
284.960431	8000.515719	9.641344	-0.058356	4.816179
284.973719	8000.529861	9.646349	-0.058359	4.816183
284.978886	8000.498975	9.651354	-0.058360	4.816174
285.075831	8000.526394	9.656359	-0.058378	4.816182
284.943930	8000.510111	9.661363	-0.058354	4.816178
285.021044	8000.432449	9.666368	-0.058368	4.816155
284.869956	8000.516264	9.671373	-0.058340	4.816180
284.970449	8000.473221	9.676378	-0.058359	4.816167
285.192831	8000.538185	9.681383	-0.058400	4.816185
285.190322	8000.477239	9.686387	-0.058400	4.816167
285.115118	8000.400011	9.691392	-0.058386	4.816145
285.217745	8000.578204	9.696397	-0.058405	4.816196
285.263157	8000.448671	9.701402	-0.058414	4.816158
285.376505	8000.527681	9.706407	-0.058435	4.816181
285.150805	8000.506486	9.711411	-0.058393	4.816176
285.318488	8000.510614	9.716416	-0.058424	4.816176
285.405670	8000.490838	9.721421	-0.058441	4.816170
285.436566	8000.496752	9.726426	-0.058447	4.816171
285.370542	8000.498766	9.731431	-0.058434	4.816172
285.195382	8000.588555	9.736435	-0.058402	4.816199
285.250192	8000.498731	9.741440	-0.058412	4.816173
285.163682	8000.522812	9.746445	-0.058396	4.816180
285.236934	8000.395923	9.751450	-0.058410	4.816143
285.240746	8000.490037	9.756455	-0.058411	4.816170
285.134738	8000.433620	9.761459	-0.058391	4.816154
285.392890	8000.443669	9.766464	-0.058439	4.816156
285.353684	8000.500668	9.771469	-0.058432	4.816173
285.367066	8000.510538	9.776474	-0.058435	4.816176
285.375964	8000.528875	9.781479	-0.058436	4.816181
285.362146	8000.458106	9.786483	-0.058434	4.816160
285.384670	8000.296100	9.791488	-0.058438	4.816113
285.393965	8000.455497	9.796493	-0.058440	4.816159
285.423005	8000.482749	9.801498	-0.058446	4.816167
285.516253	8000.488729	9.806503	-0.058463	4.816168
285.287173	8000.587155	9.811507	-0.058420	4.816198
285.268789	8000.413717	9.816512	-0.058417	4.816148
285.357587	8000.448468	9.821517	-0.058434	4.816158
285.519575	8000.373418	9.826522	-0.058464	4.816135
285.428652	8000.348264	9.831527	-0.058447	4.816128
285.380154	8000.507679	9.836531	-0.058438	4.816175
285.449353	8000.505741	9.841536	-0.058451	4.816174
285.475508	8000.414327	9.846541	-0.058456	4.816147
285.395951	8000.465249	9.851546	-0.058441	4.816162
285.590644	8000.507271	9.856551	-0.058478	4.816173
285.372398	8000.481936	9.861555	-0.058437	4.816167
285.518802	8000.383093	9.866560	-0.058464	4.816138
285.442015	8000.533445	9.871565	-0.058450	4.816182
285.491035	8000.421075	9.876570	-0.058460	4.816149
285.519405	8000.385268	9.881575	-0.058465	4.816138
285.537506	8000.483917	9.886579	-0.058468	4.816167
285.671033	8000.501317	9.891584	-0.058493	4.816171
285.538413	8000.495706	9.896589	-0.058469	4.816170
285.537847	8000.388846	9.901594	-0.058469	4.816139
285.717402	8000.511805	9.906599	-0.058502	4.816174
285.515065	8000.522023	9.911603	-0.058465	4.816178
285.445833	8000.407502	9.916608	-0.058452	4.816145
285.664544	8000.443548	9.921613	-0.058493	4.816154
285.730368	8000.403080	9.926618	-0.058505	4.816142
285.550224	8000.494916	9.931623	-0.058472	4.816170
285.465020	8000.467728	9.936627	-0.058456	4.816163
285.790501	8000.320851	9.941632	-0.058516	4.816118
285.895309	8000.377265	9.946637	-0.058536	4.816134
285.825157	8000.383478	9.951642	-0.058523	4.816136
285.896612	8000.402954	9.956647	-0.058536	4.816141
285.697090	8000.507260	9.961651	-0.058500	4.816173
285.673414	8000.348686	9.966656	-0.058495	4.816127
285.803686	8000.398084	9.971661	-0.058519	4.816140
285.709792	8000.503244	9.976666	-0.058502	4.816172
285.461241	8000.371567	9.981671	-0.058456	4.816134
285.653228	8000.505438	9.986675	-0.058492	4.816173
285.804003	8000.460104	9.991680	-0.058520	4.816158
285.655467	8000.570682	9.996685	-0.058492	4.816192
285.684649	8000.512449	10.001690	-0.058498	4.816174
285.916608	8000.423711	10.006695	-0.058541	4.816147
285.772095	8000.515127	10.011699	-0.058514	4.816175
285.756129	8000.429357	10.016704	-0.058511	4.816150
285.736304	8000.442897	10.021709	-0.058508	4.816154
285.642953	8000.467922	10.026714	-0.058491	4.816162
285.787711	8000.495144	10.031719	-0.058518	4.816169
285.771457	8000.581414	10.036723	-0.058515	4.816194
285.879513	8000.420962	10.041728	-0.058535	4.816147
285.802000	8000.442001	10.046733	-0.058521	4.816153
285.941384	8000.492634	10.051738	-0.058547	4.816167
285.900841	8000.512208	10.056743	-0.058539	4.816173
285.749292	8000.428245	10.061747	-0.058511	4.816149
285.897059	8000.426669	10.066752	-0.058539	4.816148
285.838168	8000.508957	10.071757	-0.058528	4.816173
285.897742	8000.495090	10.076762	-0.058539	4.816168
285.716553	8000.428754	10.081767	-0.058505	4.816150
285.867198	8000.525542	10.086771	-0.058533	4.816177
286.029275	8000.439807	10.091776	-0.058564	4.816151
285.882872	8000.517296	10.096781	-0.058537	4.816175
285.778496	8000.511131	10.101786	-0.058517	4.816173
286.043351	8000.372768	10.106791	-0.058567	4.816132
286.066234	8000.399908	10.111795	-0.058571	4.816139
286.017024	8000.373375	10.116800	-0.058562	4.816132
286.036596	8000.470983	10.121805	-0.058566	4.816160
285.909470	8000.505011	10.126810	-0.058542	4.816171
286.129573	8000.502615	10.131815	-0.058583	4.816169
285.813693	8000.497943	10.136819	-0.058524	4.816169
285.832916	8000.358315	10.141824	-0.058528	4.816128
286.108575	8000.433869	10.146829	-0.058579	4.816149
286.124685	8000.465161	10.151834	-0.058583	4.816158
286.141813	8000.437698	10.156839	-0.058586	4.816150
285.794279	8000.509389	10.161843	-0.058521	4.816173
285.838086	8000.501647	10.166848	-0.058530	4.816170
285.734882	8000.520081	10.171853	-0.058510	4.816176
285.938867	8000.594331	10.176858	-0.058549	4.816197
286.100020	8000.503236	10.181863	-0.058579	4.816169
286.070521	8000.586060	10.186867	-0.058573	4.816194
286.301728	8000.502651	10.191872	-0.058616	4.816168
286.227680	8000.514136	10.196877	-0.058603	4.816172
286.007589	8000.424650	10.201882	-0.058562	4.816147
286.101623	8000.363323	10.206887	-0.058579	4.816128
285.927800	8000.490538	10.211891	-0.058547	4.816167
285.933315	8000.509882	10.216896	-0.058548	4.816172
286.186313	8000.502741	10.221901	-0.058595	4.816169
286.144742	8000.487033	10.226906	-0.058588	4.816164
286.289571	8000.561276	10.231911	-0.058615	4.816185
285.865846	8000.559983	10.236915	-0.058536	4.816187
286.062586	8000.511211	10.241920	-0.058573	4.816172
285.908788	8000.515901	10.246925	-0.058544	4.816174
285.831222	8000.589301	10.251930	-0.058530	4.816196
285.932763	8000.426593	10.256935	-0.058549	4.816148
286.001741	8000.495179	10.261939	-0.058562	4.816168
286.127686	8000.403443	10.266944	-0.058585	4.816140
285.993775	8000.392466	10.271949	-0.058560	4.816138
286.147941	8000.418791	10.276954	-0.058589	4.816144
286.356263	8000.399082	10.281959	-0.058628	4.816138
286.075876	8000.478408	10.286963	-0.058576	4.816162
286.232415	8000.522942	10.291968	-0.058605	4.816174
286.105225	8000.507812	10.296973	-0.058582	4.816171
286.127431	8000.578754	10.301978	-0.058586	4.816191
286.102723	8000.513128	10.306983	-0.058581	4.816172
286.169262	8000.590220	10.311987	-0.058594	4.816194
286.142543	8000.432656	10.316992	-0.058589	4.816148
286.045064	8000.409519	10.321997	-0.058571	4.816142
286.059172	8000.586105	10.327002	-0.058574	4.816194
286.098387	8000.408370	10.332007	-0.058581	4.816142
286.044896	8000.534570	10.337011	-0.058571	4.816179
286.405997	8000.293234	10.342016	-0.058638	4.816106
286.385638	8000.504458	10.347021	-0.058635	4.816168
286.141158	8000.504291	10.352026	-0.058589	4.816169
286.194957	8000.448643	10.357031	-0.058599	4.816153
286.154576	8000.310067	10.362035	-0.058592	4.816113
286.298435	8000.339409	10.367040	-0.058619	4.816120
286.211851	8000.407302	10.372045	-0.058603	4.816141
286.438881	8000.379385	10.377050	-0.058645	4.816131
286.261835	8000.334496	10.382055	-0.058612	4.816119
286.361513	8000.427151	10.387059	-0.058631	4.816146
286.558925	8000.298245	10.392064	-0.058668	4.816107
286.436665	8000.409302	10.397069	-0.058645	4.816140
286.085456	8000.475583	10.402074	-0.058580	4.816161
286.132096	8000.421942	10.407079	-0.058589	4.816145
286.245070	8000.518046	10.412083	-0.058610	4.816173
286.279503	8000.374419	10.417088	-0.058616	4.816131
286.162088	8000.433201	10.422093	-0.058595	4.816148
286.249326	8000.502121	10.427098	-0.058611	4.816168
286.278096	8000.329539	10.432103	-0.058616	4.816118
286.211286	8000.391379	10.437107	-0.058604	4.816136
286.146215	8000.255560	10.442112	-0.058592	4.816097
286.215976	8000.392551	10.447117	-0.058605	4.816136
286.104494	8000.455716	10.452122	-0.058584	4.816155
286.317980	8000.195666	10.457127	-0.058624	4.816078
286.347536	8000.464433	10.462131	-0.058630	4.816157
286.176332	8000.367288	10.467136	-0.058598	4.816129
286.194789	8000.416789	10.472141	-0.058602	4.816143
286.132271	8000.427415	10.477146	-0.058590	4.816147
286.144103	8000.341082	10.482151	-0.058592	4.816122
286.091077	8000.439506	10.487155	-0.058583	4.816151
286.361867	8000.401700	10.492160	-0.058633	4.816138
286.362861	8000.589804	10.497165	-0.058633	4.816193
286.390834	8000.495215	10.502170	-0.058639	4.816165
286.436000	8000.376361	10.507175	-0.058647	4.816130
286.513631	8000.495331	10.512179	-0.058662	4.816165
286.490445	8000.481026	10.517184	-0.058657	4.816161
286.251980	8000.573938	10.522189	-0.058613	4.816189
286.354127	8000.492454	10.527194	-0.058632	4.816165
286.470139	8000.394125	10.532199	-0.058654	4.816135
286.315459	8000.598630	10.537203	-0.058625	4.816196
286.465646	8000.339562	10.542208	-0.058653	4.816119
286.633603	8000.407814	10.547213	-0.058685	4.816138
286.326450	8000.402232	10.552218	-0.058628	4.816138
286.320457	8000.326260	10.557223	-0.058626	4.816116
286.318615	8000.314481	10.562227	-0.058626	4.816113
286.303674	8000.324904	10.567232	-0.058623	4.816116
286.267761	8000.406543	10.572237	-0.058617	4.816140
286.369684	8000.396652	10.577242	-0.058636	4.816137
286.469002	8000.427322	10.582247	-0.058655	4.816145
286.252148	8000.513147	10.587251	-0.058614	4.816171
286.629233	8000.525364	10.592256	-0.058685	4.816173
286.392332	8000.500756	10.597261	-0.058641	4.816167
286.412816	8000.404963	10.602266	-0.058645	4.816139
286.431789	8000.366847	10.607271	-0.058648	4.816128
286.406823	8000.532037	10.612275	-0.058644	4.816176
286.662770	8000.228944	10.617280	-0.058691	4.816086
286.637298	8000.328939	10.622285	-0.058687	4.816115
286.468108	8000.292741	10.627290	-0.058655	4.816106
286.522536	8000.401671	10.632295	-0.058665	4.816137
286.577900	8000.490315	10.637299	-0.058676	4.816163
286.563188	8000.517840	10.642304	-0.058673	4.816171
286.587733	8000.429600	10.647309	-0.058678	4.816145
286.611020	8000.461023	10.652314	-0.058682	4.816154
286.452369	8000.520124	10.657319	-0.058653	4.816172
286.402343	8000.576928	10.662323	-0.058644	4.816189
286.667029	8000.404364	10.667328	-0.058693	4.816137
286.449809	8000.535065	10.672333	-0.058653	4.816177
286.486753	8000.437434	10.677338	-0.058660	4.816148
286.661891	8000.407504	10.682343	-0.058692	4.816138
286.381758	8000.526373	10.687347	-0.058640	4.816174
286.586394	8000.392255	10.692352	-0.058678	4.816134
286.746626	8000.227408	10.697357	-0.058708	4.816085
286.578360	8000.323736	10.702362	-0.058677	4.816114
286.637215	8000.200857	10.707367	-0.058688	4.816078
286.534419	8000.476835	10.712371	-0.058669	4.816159
286.763676	8000.381636	10.717376	-0.058712	4.816130
286.704216	8000.506660	10.722381	-0.058701	4.816167
286.594728	8000.591234	10.727386	-0.058681	4.816192
286.641806	8000.502336	10.732391	-0.058690	4.816166
286.780909	8000.490985	10.737395	-0.058716	4.816162
286.838506	8000.368082	10.742400	-0.058726	4.816126
286.715276	8000.366916	10.747405	-0.058703	4.816126
286.641846	8000.523745	10.752410	-0.058690	4.816172
286.704103	8000.424437	10.757415	-0.058702	4.816143
286.870032	8000.465937	10.762419	-0.058733	4.816154
286.676422	8000.452804	10.767424	-0.058697	4.816151
286.848091	8000.440977	10.772429	-0.058729	4.816147
286.722010	8000.580818	10.777434	-0.058705	4.816188
286.764619	8000.368946	10.782439	-0.058713	4.816126
286.730641	8000.526493	10.787443	-0.058707	4.816173
286.808863	8000.416789	10.792448	-0.058722	4.816140
286.773938	8000.500584	10.797453	-0.058715	4.816165
286.835170	8000.454688	10.802458	-0.058727	4.816151
286.860384	8000.152737	10.807463	-0.058731	4.816063
286.726253	8000.496537	10.812467	-0.058707	4.816164
286.904640	8000.429264	10.817472	-0.058740	4.816143
286.956586	8000.378925	10.822477	-0.058750	4.816128
286.724794	8000.504018	10.827482	-0.058707	4.816166
286.860274	8000.419935	10.832487	-0.058732	4.816141
286.872653	8000.416963	10.837491	-0.058734	4.816140
286.907339	8000.335320	10.842496	-0.058741	4.816116
286.868478	8000.413699	10.847501	-0.058734	4.816139
286.723392	8000.309548	10.852506	-0.058707	4.816109
286.753191	8000.134847	10.857511	-0.058712	4.816058
286.664005	8000.339475	10.862515	-0.058696	4.816118
286.736655	8000.317297	10.867520	-0.058710	4.816111
286.776405	8000.308412	10.872525	-0.058717	4.816109
286.552831	8000.428311	10.877530	-0.058676	4.816145
286.581062	8000.252512	10.882535	-0.058681	4.816093
286.530913	8000.509145	10.887539	-0.058672	4.816168
286.621489	8000.395392	10.892544	-0.058689	4.816135
286.712585	8000.507128	10.897549	-0.058706	4.816167
286.729294	8000.502098	10.902554	-0.058709	4.816165
286.597893	8000.365068	10.907559	-0.058685	4.816126
286.535836	8000.423790	10.912563	-0.058673	4.816143
286.823474	8000.377742	10.917568	-0.058727	4.816128
286.826355	8000.506038	10.922573	-0.058727	4.816166
286.532514	8000.559472	10.927578	-0.058673	4.816183
286.695152	8000.350854	10.932583	-0.058703	4.816121
286.804960	8000.490715	10.937587	-0.058724	4.816162
286.617155	8000.421050	10.942592	-0.058689	4.816142
286.640001	8000.466357	10.947597	-0.058693	4.816155
286.632635	8000.468369	10.952602	-0.058692	4.816156
286.684601	8000.412687	10.957607	-0.058702	4.816139
286.525796	8000.515599	10.962611	-0.058672	4.816170
286.561055	8000.524799	10.967616	-0.058679	4.816173
286.423401	8000.340637	10.972621	-0.058653	4.816120
286.486168	8000.582228	10.977626	-0.058665	4.816190
286.578251	8000.329581	10.982631	-0.058682	4.816116
286.596154	8000.432504	10.987635	-0.058686	4.816146
286.639894	8000.458956	10.992640	-0.058694	4.816153
286.710500	8000.384378	10.997645	-0.058707	4.816131
286.721217	8000.496788	11.002650	-0.058709	4.816164
286.822275	8000.471921	11.007655	-0.058728	4.816156
286.790853	8000.557917	11.012659	-0.058723	4.816181
286.819578	8000.398155	11.017664	-0.058728	4.816134
286.855976	8000.508895	11.022669	-0.058735	4.816167
286.652670	8000.504134	11.027674	-0.058697	4.816166
286.730031	8000.423267	11.032679	-0.058712	4.816142
286.995361	8000.515735	11.037683	-0.058761	4.816168
286.770712	8000.336399	11.042688	-0.058719	4.816117
286.715372	8000.451880	11.047693	-0.058709	4.816151
286.734772	8000.493919	11.052698	-0.058713	4.816163
286.862868	8000.408633	11.057703	-0.058737	4.816137
286.586762	8000.582075	11.062707	-0.058685	4.816189
286.746475	8000.490953	11.067712	-0.058715	4.816162
286.887512	8000.353540	11.072717	-0.058742	4.816121
286.962325	8000.476735	11.077722	-0.058756	4.816157
286.954405	8000.427442	11.082727	-0.058754	4.816142
287.028140	8000.409559	11.087731	-0.058768	4.816137
286.928864	8000.226094	11.092736	-0.058750	4.816084
286.751512	8000.313707	11.097741	-0.058717	4.816110
286.790051	8000.591193	11.102746	-0.058724	4.816191
286.930751	8000.355459	11.107751	-0.058750	4.816121
286.756194	8000.392898	11.112755	-0.058718	4.816133
286.820827	8000.206007	11.117760	-0.058730	4.816078
286.926171	8000.393873	11.122765	-0.058750	4.816133
286.831693	8000.396436	11.127770	-0.058732	4.816134
286.932931	8000.327759	11.132775	-0.058751	4.816113
286.734445	8000.360488	11.137779	-0.058714	4.816124
286.731192	8000.272811	11.142784	-0.058714	4.816098
286.701200	8000.414401	11.147789	-0.058708	4.816140
286.761952	8000.482839	11.152794	-0.058720	4.816159
286.861940	8000.486806	11.157799	-0.058738	4.816160
286.774147	8000.510864	11.162803	-0.058722	4.816168
286.824151	8000.386754	11.167808	-0.058732	4.816131
287.016845	8000.371036	11.172813	-0.058767	4.816125
286.703562	8000.499988	11.177818	-0.058709	4.816165
286.816853	8000.340697	11.182823	-0.058730	4.816118
286.913122	8000.501684	11.187827	-0.058749	4.816164
286.942914	8000.523608	11.192832	-0.058754	4.816170
286.883786	8000.351560	11.197837	-0.058743	4.816120
286.802407	8000.481529	11.202842	-0.058728	4.816159
287.022259	8000.244031	11.207847	-0.058769	4.816088
286.927404	8000.354519	11.212851	-0.058752	4.816121
286.652218	8000.242657	11.217856	-0.058700	4.816090
286.753684	8000.400531	11.222861	-0.058719	4.816135
286.771830	8000.493841	11.227866	-0.058723	4.816163
286.882035	8000.520435	11.232871	-0.058744	4.816170
286.800487	8000.511478	11.237875	-0.058728	4.816168
287.012787	8000.462990	11.242880	-0.058768	4.816152
286.932924	8000.489329	11.247885	-0.058753	4.816160
286.874025	8000.491472	11.252890	-0.058742	4.816161
286.896291	8000.530357	11.257895	-0.058747	4.816173
286.958309	8000.514397	11.262899	-0.058758	4.816168
287.000788	8000.579298	11.267904	-0.058766	4.816186
287.144482	8000.401324	11.272909	-0.058793	4.816133
287.159410	8000.583274	11.277914	-0.058796	4.816187
287.141516	8000.501740	11.282919	-0.058793	4.816163
287.068048	8000.512166	11.287923	-0.058779	4.816166
287.070195	8000.483361	11.292928	-0.058780	4.816158
286.887443	8000.534543	11.297933	-0.058746	4.816174
286.723709	8000.518747	11.302938	-0.058715	4.816170
286.852176	8000.409957	11.307943	-0.058739	4.816138
286.936958	8000.529060	11.312947	-0.058755	4.816172
286.808290	8000.494667	11.317952	-0.058731	4.816163
286.816380	8000.519402	11.322957	-0.058733	4.816170
286.956501	8000.486697	11.327962	-0.058759	4.816159
287.021558	8000.425910	11.332967	-0.058771	4.816141
286.941185	8000.500328	11.337971	-0.058757	4.816163
287.082889	8000.404603	11.342976	-0.058783	4.816135
287.048769	8000.438187	11.347981	-0.058777	4.816145
286.990147	8000.495904	11.352986	-0.058766	4.816162
287.098712	8000.279889	11.357991	-0.058786	4.816098
287.000036	8000.344356	11.362995	-0.058768	4.816118
286.907699	8000.386498	11.368000	-0.058751	4.816130
286.986890	8000.336655	11.373005	-0.058766	4.816115
286.827988	8000.504751	11.378010	-0.058736	4.816165
287.135393	8000.290220	11.383015	-0.058793	4.816101
287.039142	8000.440222	11.388019	-0.058776	4.816145
286.986414	8000.355917	11.393024	-0.058766	4.816121
287.053581	8000.395620	11.398029	-0.058778	4.816132
286.936459	8000.595468	11.403034	-0.058757	4.816191
287.023935	8000.401510	11.408039	-0.058773	4.816134
287.052863	8000.520664	11.413043	-0.058779	4.816169
287.077000	8000.361886	11.418048	-0.058783	4.816122
287.105568	8000.389131	11.423053	-0.058789	4.816130
286.947029	8000.513421	11.428058	-0.058759	4.816167
287.062603	8000.300739	11.433063	-0.058781	4.816104
286.964466	8000.525511	11.438067	-0.058763	4.816171
287.043115	8000.481001	11.443072	-0.058777	4.816157
287.185912	8000.402394	11.448077	-0.058804	4.816133
286.942330	8000.572155	11.453082	-0.058759	4.816184
286.979472	8000.515134	11.458087	-0.058766	4.816168
287.058499	8000.579632	11.463091	-0.058781	4.816186
286.951986	8000.465495	11.468096	-0.058761	4.816153
286.983391	8000.348526	11.473101	-0.058767	4.816119
287.184067	8000.477219	11.478106	-0.058804	4.816155
287.090132	8000.437047	11.483111	-0.058787	4.816144
287.105176	8000.526027	11.488115	-0.058790	4.816170
287.104905	8000.476873	11.493120	-0.058790	4.816156
287.238702	8000.507104	11.498125	-0.058815	4.816164
287.200861	8000.495737	11.503130	-0.058808	4.816161
287.258189	8000.389926	11.508135	-0.058819	4.816129
287.267784	8000.523690	11.513139	-0.058821	4.816168
287.157805	8000.523833	11.518144	-0.058800	4.816169
287.199158	8000.521389	11.523149	-0.058808	4.816168
287.187282	8000.561791	11.528154	-0.058806	4.816180
287.226336	8000.527246	11.533159	-0.058813	4.816170
287.034729	8000.503461	11.538163	-0.058778	4.816164
287.001982	8000.518903	11.543168	-0.058772	4.816168
287.300548	8000.389701	11.548173	-0.058827	4.816129
287.117788	8000.510344	11.553178	-0.058793	4.816165
287.205777	8000.484171	11.558183	-0.058810	4.816157
287.130143	8000.499901	11.563187	-0.058796	4.816162
287.338704	8000.501570	11.568192	-0.058835	4.816162
287.274907	8000.518585	11.573197	-0.058823	4.816167
287.187578	8000.582191	11.578202	-0.058807	4.816186
287.561144	8000.387029	11.583207	-0.058876	4.816127
287.419438	8000.462468	11.588211	-0.058850	4.816150
287.493394	8000.501227	11.593216	-0.058864	4.816161
287.529098	8000.360825	11.598221	-0.058871	4.816119
287.409674	8000.402474	11.603226	-0.058849	4.816132
287.244750	8000.412303	11.608231	-0.058818	4.816136
287.269483	8000.510009	11.613235	-0.058823	4.816164
287.027181	8000.501331	11.618240	-0.058778	4.816163
287.120459	8000.506244	11.623245	-0.058795	4.816164
287.115267	8000.500816	11.628250	-0.058794	4.816163
287.145654	8000.427642	11.633255	-0.058800	4.816141
287.152531	8000.529297	11.638259	-0.058801	4.816171
287.315353	8000.410446	11.643264	-0.058832	4.816135
287.490563	8000.397616	11.648269	-0.058864	4.816130
287.168875	8000.510386	11.653274	-0.058805	4.816165
287.383131	8000.202255	11.658279	-0.058844	4.816074
287.561231	8000.479078	11.663283	-0.058878	4.816154
287.472254	8000.377014	11.668288	-0.058861	4.816124
287.447441	8000.386189	11.673293	-0.058857	4.816127
287.279172	8000.423742	11.678298	-0.058826	4.816139
287.167827	8000.372567	11.683303	-0.058805	4.816125
287.297499	8000.450810	11.688307	-0.058829	4.816147
287.246089	8000.506521	11.693312	-0.058820	4.816163
287.309828	8000.298238	11.698317	-0.058832	4.816102
287.155027	8000.387331	11.703322	-0.058803	4.816129
287.456609	8000.331919	11.708327	-0.058859	4.816111
287.382513	8000.469502	11.713331	-0.058846	4.816152
287.240665	8000.495781	11.718336	-0.058819	4.816160
287.384861	8000.488798	11.723341	-0.058846	4.816158
287.334821	8000.497514	11.728346	-0.058837	4.816160
287.545934	8000.219246	11.733351	-0.058876	4.816078
287.374450	8000.508940	11.738355	-0.058845	4.816163
287.280467	8000.520061	11.743360	-0.058827	4.816167
287.498994	8000.339175	11.748365	-0.058868	4.816113
287.485102	8000.529149	11.753370	-0.058865	4.816169
287.241415	8000.422131	11.758375	-0.058820	4.816139
287.195701	8000.384974	11.763379	-0.058812	4.816128
287.518764	8000.449641	11.768384	-0.058872	4.816145
287.462961	8000.428329	11.773389	-0.058862	4.816139
287.288905	8000.404865	11.778394	-0.058829	4.816133
287.296014	8000.268218	11.783399	-0.058831	4.816094
287.328198	8000.534904	11.788403	-0.058837	4.816171
287.298479	8000.583530	11.793408	-0.058831	4.816186
287.517231	8000.443255	11.798413	-0.058872	4.816143
287.360432	8000.579333	11.803418	-0.058843	4.816184
287.488251	8000.430990	11.808423	-0.058867	4.816140
287.505821	8000.516811	11.813427	-0.058870	4.816165
287.483563	8000.439472	11.818432	-0.058866	4.816143
287.362115	8000.468260	11.823437	-0.058844	4.816152
287.438949	8000.605387	11.828442	-0.058858	4.816191
287.505797	8000.309530	11.833447	-0.058871	4.816104
287.456924	8000.486044	11.838451	-0.058862	4.816156
287.302954	8000.502484	11.843456	-0.058833	4.816162
287.441986	8000.257101	11.848461	-0.058859	4.816089
287.459410	8000.466880	11.853466	-0.058862	4.816151
287.533522	8000.408395	11.858471	-0.058876	4.816133
287.566230	8000.510521	11.863475	-0.058883	4.816163
287.527985	8000.367704	11.868480	-0.058875	4.816121
287.395425	8000.389877	11.873485	-0.058851	4.816128
287.199421	8000.492112	11.878490	-0.058815	4.816159
287.369485	8000.527278	11.883495	-0.058846	4.816169
287.429388	8000.494181	11.888499	-0.058858	4.816159
287.341441	8000.517168	11.893504	-0.058841	4.816166
287.618106	8000.312761	11.898509	-0.058893	4.816105
287.588458	8000.505655	11.903514	-0.058887	4.816161
287.542968	8000.262253	11.908519	-0.058879	4.816090
287.669804	8000.379985	11.913523	-0.058903	4.816124
287.565199	8000.244509	11.918528	-0.058883	4.816085
287.463843	8000.146496	11.923533	-0.058864	4.816057
287.353143	8000.532405	11.928538	-0.058844	4.816170
287.644744	8000.282318	11.933543	-0.058898	4.816096
287.619837	8000.340649	11.938547	-0.058894	4.816113
287.391035	8000.479690	11.943552	-0.058851	4.816155
287.561914	8000.424035	11.948557	-0.058883	4.816138
287.410493	8000.595476	11.953562	-0.058855	4.816188
287.499059	8000.494508	11.958567	-0.058872	4.816158
287.521706	8000.409438	11.963571	-0.058876	4.816133
287.554099	8000.526519	11.968576	-0.058882	4.816168
287.621015	8000.398440	11.973581	-0.058895	4.816130
287.443656	8000.600400	11.978586	-0.058862	4.816190
287.505632	8000.424142	11.983591	-0.058873	4.816138
287.640854	8000.331504	11.988595	-0.058899	4.816110
287.353273	8000.325208	11.993600	-0.058845	4.816110
287.603619	8000.462288	11.998605	-0.058892	4.816148
287.589079	8000.403256	12.003610	-0.058889	4.816131
287.756870	8000.196867	12.008615	-0.058921	4.816070
287.461102	8000.366747	12.013619	-0.058866	4.816121
287.530635	8000.539006	12.018624	-0.058879	4.816171
287.625334	8000.429600	12.023629	-0.058896	4.816139
287.382977	8000.564119	12.028634	-0.058852	4.816179
287.429703	8000.411094	12.033639	-0.058860	4.816134
287.503632	8000.502216	12.038643	-0.058874	4.816161
287.358472	8000.524160	12.043648	-0.058847	4.816168
287.547281	8000.383341	12.048653	-0.058882	4.816126
287.531251	8000.495266	12.053658	-0.058880	4.816158
287.603403	8000.323468	12.058663	-0.058893	4.816108
287.429898	8000.494506	12.063667	-0.058861	4.816159
287.633437	8000.404181	12.068672	-0.058899	4.816131
287.933459	8000.427822	12.073677	-0.058955	4.816137
287.599675	8000.500832	12.078682	-0.058893	4.816160
287.629804	8000.508870	12.083687	-0.058898	4.816162
287.655864	8000.369360	12.088691	-0.058903	4.816121
287.545632	8000.561856	12.093696	-0.058883	4.816178
287.528423	8000.299733	12.098701	-0.058880	4.816101
287.570920	8000.381733	12.103706	-0.058888	4.816125
287.696573	8000.313500	12.108711	-0.058911	4.816104
287.561079	8000.440347	12.113715	-0.058886	4.816142
287.405148	8000.425761	12.118720	-0.058857	4.816139
287.552402	8000.503258	12.123725	-0.058885	4.816161
287.533255	8000.428112	12.128730	-0.058881	4.816139
287.525260	8000.519880	12.133735	-0.058880	4.816166
287.678142	8000.254443	12.138739	-0.058908	4.816087
287.494297	8000.505441	12.143744	-0.058874	4.816162
287.693911	8000.526185	12.148749	-0.058912	4.816167
287.659199	8000.496708	12.153754	-0.058905	4.816158
287.714031	8000.490235	12.158759	-0.058916	4.816156
287.459403	8000.515528	12.163763	-0.058868	4.816165
287.500983	8000.492784	12.168768	-0.058876	4.816158
287.568345	8000.521805	12.173773	-0.058889	4.816166
287.384724	8000.446871	12.178778	-0.058855	4.816145
287.295964	8000.402517	12.183783	-0.058838	4.816133
287.638155	8000.316855	12.188787	-0.058902	4.816106
287.523046	8000.420563	12.193792	-0.058881	4.816137
287.668911	8000.355904	12.198797	-0.058908	4.816117
287.489632	8000.515082	12.203802	-0.058875	4.816164
287.422092	8000.328986	12.208807	-0.058862	4.816110
287.371838	8000.525779	12.213811	-0.058853	4.816168
287.428280	8000.501168	12.218816	-0.058863	4.816161
287.441912	8000.506769	12.223821	-0.058866	4.816162
287.482463	8000.568430	12.228826	-0.058874	4.816180
287.626772	8000.372298	12.233831	-0.058901	4.816122
287.702577	8000.504063	12.238835	-0.058915	4.816160
287.648771	8000.495611	12.243840	-0.058905	4.816158
287.675363	8000.391377	12.248845	-0.058910	4.816127
287.657223	8000.417772	12.253850	-0.058907	4.816135
287.603616	8000.390088	12.258855	-0.058897	4.816127
287.543415	8000.517239	12.263859	-0.058886	4.816165
287.598438	8000.456268	12.268864	-0.058896	4.816147
287.710686	8000.423056	12.273869	-0.058917	4.816136
287.635223	8000.524282	12.278874	-0.058903	4.816166
287.554428	8000.345423	12.283879	-0.058888	4.816114
287.446870	8000.342405	12.288883	-0.058868	4.816114
287.689312	8000.514607	12.293888	-0.058913	4.816163
287.880097	8000.422981	12.298893	-0.058949	4.816135
287.896915	8000.484210	12.303898	-0.058952	4.816153
287.499589	8000.515453	12.308903	-0.058878	4.816164
287.550566	8000.420212	12.313907	-0.058888	4.816136
287.668518	8000.516411	12.318912	-0.058910	4.816164
287.802022	8000.428016	12.323917	-0.058935	4.816137
287.626144	8000.528481	12.328922	-0.058902	4.816168
287.484624	8000.228830	12.333927	-0.058876	4.816081
287.650553	8000.457344	12.338931	-0.058907	4.816147
287.692582	8000.306370	12.343936	-0.058915	4.816102
287.505503	8000.291218	12.348941	-0.058880	4.816099
287.484508	8000.527015	12.353946	-0.058876	4.816168
287.693159	8000.338467	12.358951	-0.058915	4.816112
287.771958	8000.333499	12.363955	-0.058930	4.816110
287.521711	8000.371697	12.368960	-0.058884	4.816122
287.555556	8000.365910	12.373965	-0.058890	4.816120
287.586654	8000.516097	12.378970	-0.058896	4.816164
287.728332	8000.397928	12.383975	-0.058922	4.816129
287.679639	8000.425904	12.388979	-0.058913	4.816137
287.944639	8000.522645	12.393984	-0.058963	4.816164
287.765412	8000.360159	12.398989	-0.058929	4.816118
287.806311	8000.487014	12.403994	-0.058937	4.816154
287.757195	8000.411323	12.408999	-0.058928	4.816133
287.673612	8000.527362	12.414003	-0.058913	4.816167
287.546590	8000.464144	12.419008	-0.058889	4.816149
287.725871	8000.380857	12.424013	-0.058923	4.816124
287.646925	8000.564306	12.429018	-0.058908	4.816178
287.830241	8000.413767	12.434023	-0.058942	4.816133
287.676749	8000.435560	12.439027	-0.058914	4.816140
287.684630	8000.512655	12.444032	-0.058915	4.816163
287.742370	8000.401507	12.449037	-0.058926	4.816130
287.559991	8000.510403	12.454042	-0.058892	4.816163
287.697638	8000.346210	12.459047	-0.058918	4.816114
287.718142	8000.402162	12.464051	-0.058922	4.816130
287.597475	8000.521799	12.469056	-0.058900	4.816166
287.861941	8000.434721	12.474061	-0.058949	4.816139
287.870626	8000.469085	12.479066	-0.058951	4.816149
287.872151	8000.415689	12.484071	-0.058951	4.816133
287.905053	8000.417366	12.489075	-0.058957	4.816133
287.818547	8000.500224	12.494080	-0.058941	4.816158
287.818137	8000.273671	12.499085	-0.058941	4.816092
287.804559	8000.291600	12.504090	-0.058939	4.816097
287.689794	8000.289519	12.509095	-0.058917	4.816097
287.796683	8000.395133	12.514099	-0.058937	4.816128
287.708598	8000.420254	12.519104	-0.058921	4.816135
287.984357	8000.242546	12.524109	-0.058972	4.816082
287.693165	8000.384726	12.529114	-0.058918	4.816125
287.749633	8000.412479	12.534119	-0.058929	4.816133
287.686112	8000.380341	12.539123	-0.058917	4.816124
287.646457	8000.490767	12.544128	-0.058910	4.816156
287.639293	8000.479959	12.549133	-0.058909	4.816153
287.603646	8000.410925	12.554138	-0.058902	4.816133
287.716792	8000.525204	12.559143	-0.058923	4.816166
287.756437	8000.344264	12.564147	-0.058931	4.816113
287.651238	8000.505861	12.569152	-0.058911	4.816161
287.786471	8000.260406	12.574157	-0.058937	4.816088
287.874790	8000.416977	12.579162	-0.058953	4.816133
287.832010	8000.372393	12.584167	-0.058945	4.816121
287.854999	8000.481823	12.589171	-0.058950	4.816153
287.807806	8000.462805	12.594176	-0.058941	4.816147
287.840850	8000.274265	12.599181	-0.058947	4.816092
287.649710	8000.266519	12.604186	-0.058912	4.816091
287.804112	8000.262927	12.609191	-0.058940	4.816089
287.686039	8000.420015	12.614195	-0.058919	4.816135
287.715393	8000.462236	12.619200	-0.058924	4.816148
287.893470	8000.393888	12.624205	-0.058957	4.816127
287.711166	8000.503854	12.629210	-0.058924	4.816160
287.878501	8000.263259	12.634215	-0.058955	4.816089
287.761259	8000.377615	12.639219	-0.058933	4.816123
287.834324	8000.386435	12.644224	-0.058947	4.816125
287.946564	8000.347880	12.649229	-0.058968	4.816113
287.915116	8000.403955	12.654234	-0.058962	4.816129
287.855600	8000.335555	12.659239	-0.058951	4.816110
287.808606	8000.514242	12.664243	-0.058942	4.816162
287.686764	8000.580426	12.669248	-0.058920	4.816182
287.731140	8000.425219	12.674253	-0.058928	4.816137
287.687376	8000.571905	12.679258	-0.058920	4.816180
287.715895	8000.500834	12.684263	-0.058926	4.816159
287.775181	8000.404675	12.689267	-0.058937	4.816130
287.726334	8000.409138	12.694272	-0.058928	4.816132
287.726774	8000.343967	12.699277	-0.058928	4.816113
287.669668	8000.522470	12.704282	-0.058917	4.816165
287.694255	8000.474837	12.709287	-0.058922	4.816151
287.879041	8000.517752	12.714291	-0.058956	4.816163
287.880874	8000.511383	12.719296	-0.058957	4.816161
287.863497	8000.476878	12.724301	-0.058954	4.816151
287.923467	8000.491872	12.729306	-0.058965	4.816155
287.992307	8000.502753	12.734311	-0.058978	4.816158
287.913772	8000.389122	12.739315	-0.058963	4.816125
287.983147	8000.456652	12.744320	-0.058976	4.816144
287.832313	8000.445364	12.749325	-0.058948	4.816142
287.532832	8000.485870	12.754330	-0.058893	4.816155
287.861745	8000.511107	12.759335	-0.058954	4.816161
287.939046	8000.417413	12.764339	-0.058969	4.816133
287.720299	8000.497861	12.769344	-0.058928	4.816158
287.718423	8000.435854	12.774349	-0.058928	4.816140
287.756763	8000.545565	12.779354	-0.058935	4.816172
287.710262	8000.470989	12.784359	-0.058926	4.816150
287.778915	8000.385688	12.789363	-0.058939	4.816125
287.788379	8000.482048	12.794368	-0.058941	4.816153
287.937410	8000.358670	12.799373	-0.058969	4.816116
287.976109	8000.463044	12.804378	-0.058976	4.816146
287.926910	8000.403381	12.809383	-0.058967	4.816129
287.878191	8000.401433	12.814387	-0.058958	4.816129
287.814090	8000.407756	12.819392	-0.058946	4.816131
287.822098	8000.411116	12.824397	-0.058948	4.816132
287.846314	8000.476755	12.829402	-0.058952	4.816151
287.928462	8000.413072	12.834407	-0.058968	4.816132
287.717592	8000.420995	12.839411	-0.058929	4.816135
287.730308	8000.486424	12.844416	-0.058931	4.816154
287.744924	8000.502729	12.849421	-0.058934	4.816159
287.733883	8000.484370	12.854426	-0.058932	4.816154
287.707506	8000.581146	12.859431	-0.058927	4.816182
287.911685	8000.584875	12.864435	-0.058965	4.816182
287.882744	8000.493520	12.869440	-0.058960	4.816156
287.866539	8000.506058	12.874445	-0.058957	4.816159
287.781088	8000.489549	12.879450	-0.058941	4.816155
288.021501	8000.522792	12.884455	-0.058986	4.816163
288.049238	8000.525443	12.889459	-0.058991	4.816164
287.857612	8000.551884	12.894464	-0.058956	4.816173
287.939726	8000.250959	12.899469	-0.058971	4.816084
288.126406	8000.523670	12.904474	-0.059006	4.816163
287.979752	8000.291246	12.909479	-0.058979	4.816096
287.992109	8000.414375	12.914483	-0.058981	4.816132
288.018226	8000.483255	12.919488	-0.058986	4.816152
287.953054	8000.241629	12.924493	-0.058974	4.816082
287.977570	8000.528485	12.929498	-0.058979	4.816165
288.044999	8000.478426	12.934503	-0.058991	4.816150
288.130679	8000.356031	12.939507	-0.059007	4.816114
287.918620	8000.486828	12.944512	-0.058968	4.816153
288.030512	8000.285831	12.949517	-0.058989	4.816094
288.068673	8000.506679	12.954522	-0.058996	4.816158
288.047583	8000.417604	12.959527	-0.058992	4.816133
288.091484	8000.562683	12.964531	-0.059001	4.816175
287.893380	8000.486414	12.969536	-0.058964	4.816153
287.962115	8000.407525	12.974541	-0.058977	4.816130
287.995148	8000.439127	12.979546	-0.058983	4.816139
288.014641	8000.499336	12.984551	-0.058987	4.816157
288.061988	8000.505551	12.989555	-0.058996	4.816158
287.791222	8000.500628	12.994560	-0.058945	4.816158
287.866831	8000.298970	12.999565	-0.058959	4.816099
287.901230	8000.269683	13.004570	-0.058966	4.816090
287.843338	8000.283599	13.009575	-0.058955	4.816094
287.989859	8000.226432	13.014579	-0.058982	4.816077
287.875902	8000.434890	13.019584	-0.058961	4.816138
288.226233	8000.329071	13.024589	-0.059027	4.816106
287.832335	8000.496097	13.029594	-0.058954	4.816157
288.023764	8000.422649	13.034599	-0.058989	4.816134
287.999958	8000.510924	13.039603	-0.058985	4.816160
288.022894	8000.388454	13.044608	-0.058989	4.816124
288.219494	8000.162283	13.049613	-0.059026	4.816057
287.954297	8000.482334	13.054618	-0.058977	4.816152
288.021674	8000.499600	13.059623	-0.058989	4.816157
288.036257	8000.495600	13.064627	-0.058992	4.816155
288.129755	8000.452428	13.069632	-0.059010	4.816142
288.115470	8000.417980	13.074637	-0.059007	4.816132
287.859976	8000.518064	13.079642	-0.058960	4.816163
287.940825	8000.391306	13.084647	-0.058975	4.816125
288.062605	8000.344375	13.089651	-0.058997	4.816111
287.750059	8000.554560	13.094656	-0.058940	4.816174
288.013454	8000.369146	13.099661	-0.058989	4.816118
288.226335	8000.431809	13.104666	-0.059028	4.816136
287.952852	8000.492024	13.109671	-0.058978	4.816155
287.965219	8000.454855	13.114675	-0.058980	4.816144
287.935065	8000.395539	13.119680	-0.058974	4.816127
288.021397	8000.408876	13.124685	-0.058990	4.816130
288.085589	8000.437839	13.129690	-0.059003	4.816138
288.119906	8000.409620	13.134695	-0.059009	4.816130
288.256662	8000.522193	13.139699	-0.059035	4.816162
288.078655	8000.520027	13.144704	-0.059002	4.816162
288.081947	8000.291403	13.149709	-0.059002	4.816095
288.189516	8000.224977	13.154714	-0.059022	4.816075
287.960605	8000.424930	13.159719	-0.058980	4.816135
288.051982	8000.336836	13.164723	-0.058997	4.816109
288.054260	8000.457645	13.169728	-0.058997	4.816144
288.161006	8000.379449	13.174733	-0.059017	4.816121
288.033218	8000.505370	13.179738	-0.058994	4.816158
287.983646	8000.507682	13.184743	-0.058985	4.816159
288.021696	8000.265799	13.189747	-0.058992	4.816088
287.975122	8000.496858	13.194752	-0.058983	4.816156
287.984761	8000.505592	13.199757	-0.058985	4.816158
288.023291	8000.471037	13.204762	-0.058992	4.816148
287.977891	8000.374040	13.209767	-0.058984	4.816120
288.084518	8000.374922	13.214771	-0.059004	4.816120
288.067156	8000.500717	13.219776	-0.059001	4.816157
288.382297	8000.426317	13.224781	-0.059060	4.816133
288.371540	8000.513762	13.229786	-0.059058	4.816159
288.223929	8000.510012	13.234791	-0.059030	4.816158
288.227097	8000.406418	13.239795	-0.059031	4.816128
288.190387	8000.498733	13.244800	-0.059024	4.816155
288.091807	8000.213751	13.249805	-0.059006	4.816073
288.213516	8000.389099	13.254810	-0.059029	4.816123
288.125247	8000.421698	13.259815	-0.059012	4.816133
287.983477	8000.410575	13.264819	-0.058986	4.816131
287.999037	8000.404455	13.269824	-0.058989	4.816129
288.284407	8000.198068	13.274829	-0.059042	4.816067
288.228558	8000.309269	13.279834	-0.059032	4.816100
288.041075	8000.282353	13.284839	-0.058997	4.816093
288.358611	8000.249674	13.289843	-0.059056	4.816082
288.000165	8000.407727	13.294848	-0.058990	4.816130
288.249186	8000.377006	13.299853	-0.059036	4.816119
288.191627	8000.475353	13.304858	-0.059026	4.816148
288.056713	8000.376724	13.309863	-0.059000	4.816120
287.980027	8000.356101	13.314867	-0.058986	4.816115
287.972185	8000.404056	13.319872	-0.058985	4.816129
288.037769	8000.342209	13.324877	-0.058997	4.816110
287.984844	8000.516515	13.329882	-0.058988	4.816162
287.874229	8000.421535	13.334887	-0.058967	4.816134
287.942485	8000.240048	13.339891	-0.058980	4.816081
287.939999	8000.344739	13.344896	-0.058979	4.816112
288.189225	8000.262726	13.349901	-0.059026	4.816086
288.283057	8000.416195	13.354906	-0.059043	4.816131
288.301846	8000.385555	13.359911	-0.059047	4.816122
288.139538	8000.336654	13.364915	-0.059017	4.816108
288.402858	8000.180092	13.369920	-0.059066	4.816061
288.385394	8000.102840	13.374925	-0.059063	4.816039
288.289772	8000.320182	13.379930	-0.059045	4.816103
288.099801	8000.420391	13.384935	-0.059010	4.816133
288.130356	8000.299129	13.389939	-0.059016	4.816097
288.033038	8000.424536	13.394944	-0.058998	4.816134
288.058115	8000.431414	13.399949	-0.059002	4.816136
288.163428	8000.343574	13.404954	-0.059022	4.816110
288.059444	8000.329933	13.409959	-0.059003	4.816107
288.175259	8000.318159	13.414963	-0.059024	4.816103
288.052893	8000.466621	13.419968	-0.059002	4.816147
288.284440	8000.330853	13.424973	-0.059045	4.816106
288.194435	8000.328154	13.429978	-0.059028	4.816105
288.162556	8000.320101	13.434983	-0.059022	4.816103
288.229465	8000.306368	13.439987	-0.059035	4.816099
288.213817	8000.346701	13.444992	-0.059032	4.816111
288.187870	8000.230822	13.449997	-0.059027	4.816077
288.224043	8000.405682	13.455002	-0.059034	4.816128
288.300083	8000.298072	13.460007	-0.059048	4.816096
288.350435	8000.298999	13.465011	-0.059058	4.816096
288.038885	8000.419435	13.470016	-0.059000	4.816133
288.427294	8000.182864	13.475021	-0.059072	4.816062
288.304873	8000.452084	13.480026	-0.059050	4.816141
288.143264	8000.457698	13.485031	-0.059020	4.816143
288.150531	8000.395857	13.490035	-0.059021	4.816125
288.060162	8000.459408	13.495040	-0.059005	4.816144
288.092076	8000.443968	13.500045	-0.059011	4.816140
288.005151	8000.339802	13.505050	-0.058994	4.816110
288.018944	8000.329376	13.510055	-0.058997	4.816107
288.002499	8000.305575	13.515059	-0.058994	4.816100
287.971863	8000.496316	13.520064	-0.058989	4.816156
288.292449	8000.385681	13.525069	-0.059048	4.816122
288.326372	8000.424780	13.530074	-0.059055	4.816133
288.017471	8000.409544	13.535079	-0.058997	4.816130
288.208878	8000.222818	13.540083	-0.059033	4.816074
288.217484	8000.414274	13.545088	-0.059035	4.816130
288.407655	8000.138827	13.550093	-0.059070	4.816049
288.211550	8000.232512	13.555098	-0.059034	4.816077
288.325538	8000.203606	13.560103	-0.059055	4.816068
288.266594	8000.166207	13.565107	-0.059044	4.816058
288.122976	8000.331379	13.570112	-0.059018	4.816107
288.127963	8000.359264	13.575117	-0.059019	4.816115
288.052295	8000.377131	13.580122	-0.059005	4.816120
288.111955	8000.518222	13.585127	-0.059016	4.816161
287.995173	8000.411374	13.590131	-0.058994	4.816131
288.225714	8000.503214	13.595136	-0.059037	4.816156
288.196447	8000.392617	13.600141	-0.059032	4.816124
288.071720	8000.429894	13.605146	-0.059009	4.816136
288.280360	8000.498893	13.610151	-0.059048	4.816155
288.190968	8000.268579	13.615155	-0.059031	4.816088
288.173588	8000.414678	13.620160	-0.059028	4.816131
288.239804	8000.247045	13.625165	-0.059040	4.816081
288.241656	8000.362503	13.630170	-0.059041	4.816115
288.188067	8000.441686	13.635175	-0.059031	4.816138
288.247076	8000.312393	13.640179	-0.059042	4.816100
288.181070	8000.316543	13.645184	-0.059030	4.816102
288.018961	8000.398023	13.650189	-0.059000	4.816127
288.220124	8000.290556	13.655194	-0.059037	4.816094
288.134560	8000.350989	13.660199	-0.059021	4.816112
288.098045	8000.215682	13.665203	-0.059015	4.816073
287.894414	8000.513343	13.670208	-0.058977	4.816161
288.193556	8000.391631	13.675213	-0.059033	4.816124
288.267384	8000.406877	13.680218	-0.059047	4.816128
288.163214	8000.371860	13.685223	-0.059027	4.816118
288.282243	8000.496934	13.690227	-0.059050	4.816154
288.358781	8000.411776	13.695232	-0.059064	4.816129
288.318834	8000.373653	13.700237	-0.059056	4.816118
288.479654	8000.407584	13.705242	-0.059087	4.816127
288.488806	8000.308373	13.710247	-0.059088	4.816098
288.380845	8000.420763	13.715251	-0.059068	4.816131
288.181705	8000.348750	13.720256	-0.059031	4.816111
288.300446	8000.421454	13.725261	-0.059054	4.816132
288.411439	8000.282421	13.730266	-0.059074	4.816091
288.081817	8000.349094	13.735271	-0.059013	4.816112
288.166641	8000.389120	13.740275	-0.059029	4.816123
288.101825	8000.405047	13.745280	-0.059017	4.816128
288.112583	8000.281288	13.750285	-0.059019	4.816092
288.080813	8000.376897	13.755290	-0.059013	4.816120
288.088424	8000.523452	13.760295	-0.059015	4.816163
288.400290	8000.314341	13.765299	-0.059073	4.816100
288.362420	8000.446175	13.770304	-0.059066	4.816139
288.515718	8000.353865	13.775309	-0.059094	4.816111
288.583570	8000.385033	13.780314	-0.059107	4.816120
288.310364	8000.508305	13.785319	-0.059057	4.816157
288.300251	8000.329662	13.790323	-0.059055	4.816105
288.239463	8000.489932	13.795328	-0.059044	4.816152
288.400818	8000.318688	13.800333	-0.059074	4.816101
288.243618	8000.419494	13.805338	-0.059044	4.816132
288.233157	8000.407557	13.810343	-0.059043	4.816128
288.305552	8000.390718	13.815347	-0.059056	4.816123
288.178636	8000.432230	13.820352	-0.059033	4.816136
288.185794	8000.431301	13.825357	-0.059034	4.816135
288.433841	8000.431554	13.830362	-0.059080	4.816134
288.126979	8000.193005	13.835367	-0.059023	4.816066
288.108798	8000.328402	13.840371	-0.059020	4.816106
288.086814	8000.397474	13.845376	-0.059016	4.816126
288.332882	8000.162585	13.850381	-0.059062	4.816056
288.237847	8000.414136	13.855386	-0.059044	4.816130
288.340346	8000.359373	13.860391	-0.059063	4.816114
288.288797	8000.260126	13.865395	-0.059054	4.816085
288.220494	8000.501478	13.870400	-0.059041	4.816156
288.338815	8000.267467	13.875405	-0.059063	4.816087
288.448339	8000.391299	13.880410	-0.059084	4.816122
288.273527	8000.276982	13.885415	-0.059051	4.816090
288.238823	8000.372539	13.890419	-0.059045	4.816118
288.313479	8000.361084	13.895424	-0.059059	4.816114
288.391450	8000.120996	13.900429	-0.059073	4.816044
288.067119	8000.225169	13.905434	-0.059013	4.816076
288.049963	8000.322113	13.910439	-0.059010	4.816104
288.195155	8000.404917	13.915443	-0.059037	4.816128
288.107598	8000.518747	13.920448	-0.059021	4.816161
288.230720	8000.387415	13.925453	-0.059044	4.816122
288.332826	8000.190513	13.930458	-0.059063	4.816064
288.382266	8000.295083	13.935463	-0.059073	4.816094
288.390044	8000.101807	13.940467	-0.059074	4.816038
288.355887	8000.407899	13.945472	-0.059068	4.816128
288.426307	8000.424153	13.950477	-0.059081	4.816132
288.251053	8000.406007	13.955482	-0.059049	4.816128
288.148260	8000.366740	13.960487	-0.059029	4.816117
288.289455	8000.386420	13.965491	-0.059056	4.816122
288.202732	8000.419047	13.970496	-0.059040	4.816132
288.274135	8000.341275	13.975501	-0.059053	4.816109
288.357926	8000.302201	13.980506	-0.059069	4.816097
288.127507	8000.491441	13.985511	-0.059026	4.816153
288.238703	8000.302185	13.990515	-0.059047	4.816097
288.243485	8000.366401	13.995520	-0.059048	4.816116
288.419944	8000.408097	14.000525	-0.059081	4.816127
288.331324	8000.428933	14.005530	-0.059064	4.816134
288.159267	8000.515576	14.010535	-0.059033	4.816160
288.416528	8000.286233	14.015539	-0.059080	4.816092
288.290165	8000.416455	14.020544	-0.059057	4.816130
288.239346	8000.385616	14.025549	-0.059048	4.816122
288.157727	8000.344597	14.030554	-0.059033	4.816110
288.239890	8000.358927	14.035559	-0.059048	4.816114
288.316402	8000.161559	14.040563	-0.059062	4.816056
288.269535	8000.333837	14.045568	-0.059054	4.816106
288.334685	8000.216411	14.050573	-0.059066	4.816072
288.190816	8000.355932	14.055578	-0.059039	4.816113
288.271695	8000.415122	14.060583	-0.059054	4.816130
288.237016	8000.061843	14.065587	-0.059048	4.816027
288.193417	8000.400890	14.070592	-0.059040	4.816126
288.244974	8000.282148	14.075597	-0.059050	4.816091
288.270358	8000.508108	14.080602	-0.059055	4.816157
288.440055	8000.408617	14.085607	-0.059086	4.816127
288.445256	8000.248420	14.090611	-0.059087	4.816080
288.136475	8000.386005	14.095616	-0.059030	4.816122
288.404607	8000.313955	14.100621	-0.059080	4.816100
288.384701	8000.380927	14.105626	-0.059076	4.816119
288.121240	8000.481935	14.110631	-0.059027	4.816150
288.454512	8000.339470	14.115635	-0.059089	4.816107
288.295501	8000.403909	14.120640	-0.059060	4.816127
288.295893	8000.240419	14.125645	-0.059060	4.816079
288.257068	8000.285674	14.130650	-0.059053	4.816092
288.203847	8000.417227	14.135655	-0.059043	4.816131
288.393409	8000.375806	14.140659	-0.059078	4.816118
288.378423	8000.414014	14.145664	-0.059076	4.816129
288.383197	8000.300831	14.150669	-0.059077	4.816096
288.473245	8000.322785	14.155674	-0.059094	4.816102
288.451134	8000.398267	14.160679	-0.059090	4.816124
288.377269	8000.192815	14.165683	-0.059076	4.816064
288.478084	8000.229926	14.170688	-0.059095	4.816075
288.319709	8000.367046	14.175693	-0.059065	4.816116
288.347698	8000.342985	14.180698	-0.059071	4.816109
288.416418	8000.245929	14.185703	-0.059083	4.816080
288.313007	8000.121159	14.190707	-0.059064	4.816044
288.364801	8000.398895	14.195712	-0.059074	4.816125
288.303327	8000.305878	14.200717	-0.059063	4.816098
288.460207	8000.395307	14.205722	-0.059092	4.816123
288.287319	8000.502240	14.210727	-0.059060	4.816155
288.402440	8000.284200	14.215731	-0.059081	4.816091
288.429808	8000.400124	14.220736	-0.059087	4.816125
288.262788	8000.387472	14.225741	-0.059056	4.816122
288.257192	8000.452568	14.230746	-0.059055	4.816141
288.168013	8000.340880	14.235751	-0.059038	4.816109
288.174277	8000.385887	14.240755	-0.059040	4.816122
288.202856	8000.409927	14.245760	-0.059045	4.816129
288.116747	8000.267304	14.250765	-0.059029	4.816088
288.266714	8000.415383	14.255770	-0.059057	4.816130
288.384950	8000.415409	14.260775	-0.059079	4.816129
288.262453	8000.264642	14.265779	-0.059056	4.816086
288.280191	8000.459471	14.270784	-0.059060	4.816143
288.323859	8000.408980	14.275789	-0.059068	4.816128
288.312450	7999.575239	14.280794	-0.059065	4.815884

288.371285	7996.269280	14.285799	-0.059074	4.814918
288.375190	7990.708197	14.290803	-0.059072	4.813293
288.140631	7983.958598	14.295808	-0.059024	4.811321
288.188354	7976.619233	14.300813	-0.059028	4.809174
288.244436	7969.055022	14.305818	-0.059033	4.806960
287.994547	7961.191552	14.310823	-0.058982	4.804659
288.011077	7953.378058	14.315827	-0.058980	4.802370
288.120634	7945.378144	14.320832	-0.058995	4.800025
288.175066	7937.476998	14.325837	-0.059000	4.797708
287.988235	7929.478850	14.330842	-0.058960	4.795363
287.949978	7921.368002	14.335847	-0.058948	4.792983
288.072584	7913.449818	14.340851	-0.058966	4.790657
287.951850	7905.392388	14.345856	-0.058938	4.788291
288.007462	7897.423535	14.350861	-0.058943	4.785948
288.020272	7889.430310	14.355866	-0.058941	4.783598
287.853884	7881.422360	14.360871	-0.058905	4.781243
287.955898	7873.444754	14.365875	-0.058918	4.778894
287.765467	7865.442298	14.370880	-0.058878	4.776538
287.826648	7857.431688	14.375885	-0.058884	4.774178
287.640884	7849.390731	14.380890	-0.058844	4.771808
287.713274	7841.351199	14.385895	-0.058853	4.769436
287.736244	7833.351970	14.390899	-0.058852	4.767076
287.483032	7825.382453	14.395904	-0.058800	4.764724
287.508815	7817.395451	14.400909	-0.058799	4.762365
287.575762	7809.414021	14.405914	-0.058807	4.760006
287.395637	7801.431118	14.410919	-0.058768	4.757646
287.254933	7793.383135	14.415923	-0.058737	4.755266
287.151328	7785.327070	14.420928	-0.058712	4.752882
287.251898	7777.290352	14.425933	-0.058726	4.750502
287.239371	7769.387900	14.430938	-0.058718	4.748161
287.049249	7761.312362	14.435943	-0.058678	4.745768
287.091709	7753.373266	14.440947	-0.058681	4.743413
287.034517	7745.380105	14.445952	-0.058665	4.741042
286.908170	7737.347050	14.450957	-0.058636	4.738657
286.798784	7729.370836	14.455962	-0.058611	4.736289
286.758159	7721.277608	14.460967	-0.058598	4.733884
286.718733	7713.320805	14.465971	-0.058586	4.731518
286.773176	7705.296639	14.470976	-0.058591	4.729131
286.898044	7697.308735	14.475981	-0.058609	4.726753
286.766255	7689.340954	14.480986	-0.058579	4.724381
286.769559	7681.324162	14.485991	-0.058575	4.721993
286.677653	7673.338733	14.490995	-0.058552	4.719613
286.621734	7665.378669	14.496000	-0.058537	4.717239
286.618351	7657.311226	14.501005	-0.058531	4.714832
286.525416	7649.305601	14.506010	-0.058509	4.712443
286.392397	7641.284892	14.511015	-0.058479	4.710048
286.303179	7633.325130	14.516019	-0.058457	4.707669
286.363278	7625.271610	14.521024	-0.058463	4.705261
286.475102	7617.335346	14.526029	-0.058479	4.702887
286.470590	7609.306100	14.531034	-0.058473	4.700484
286.334129	7601.325717	14.536039	-0.058442	4.698095
286.390183	7593.335421	14.541043	-0.058448	4.695701
286.318758	7585.299215	14.546048	-0.058429	4.693292
286.172755	7577.245768	14.551053	-0.058397	4.690877
286.231699	7569.335417	14.556058	-0.058403	4.688504
285.964062	7561.258182	14.561063	-0.058348	4.686079
286.021320	7553.297759	14.566067	-0.058353	4.683688
285.979400	7545.312640	14.571072	-0.058340	4.681289
286.053460	7537.327251	14.576077	-0.058349	4.678887
285.966806	7529.308548	14.581082	-0.058328	4.676475
285.714639	7521.227615	14.586087	-0.058276	4.674044
285.770489	7513.213055	14.591091	-0.058281	4.671630
285.722600	7505.174019	14.596096	-0.058267	4.669208
285.614507	7497.240291	14.601101	-0.058242	4.666817
285.878374	7489.254862	14.606106	-0.058286	4.664408
285.793306	7481.239468	14.611111	-0.058265	4.661989
285.712834	7473.258278	14.616115	-0.058245	4.659579
285.519455	7465.260011	14.621120	-0.058203	4.657164
285.695464	7457.249218	14.626125	-0.058231	4.654742
285.648413	7449.210508	14.631130	-0.058217	4.652311
285.318209	7441.157198	14.636135	-0.058151	4.649875
285.277187	7433.244577	14.641139	-0.058138	4.647480
285.287827	7425.235282	14.646144	-0.058135	4.645054
285.182309	7417.261644	14.651149	-0.058110	4.642638
285.132319	7409.231678	14.656154	-0.058095	4.640204
285.129516	7401.260655	14.661159	-0.058090	4.637786
285.419594	7393.256742	14.666163	-0.058139	4.635356
285.078687	7385.185013	14.671168	-0.058070	4.632905
285.106752	7377.189685	14.676173	-0.058070	4.630476
285.005444	7369.203321	14.681178	-0.058046	4.628048
284.941762	7361.178194	14.686183	-0.058029	4.625608
284.949580	7353.241612	14.691187	-0.058026	4.623192
284.946791	7345.206647	14.696192	-0.058020	4.620746
284.891182	7337.195306	14.701197	-0.058004	4.618306
284.961896	7329.207918	14.706202	-0.058013	4.615871
284.947548	7321.174435	14.711207	-0.058005	4.613421
284.849991	7313.164549	14.716211	-0.057981	4.610977
284.601445	7305.156726	14.721216	-0.057930	4.608533
284.744798	7297.149577	14.726221	-0.057952	4.606087
284.931043	7289.230418	14.731226	-0.057981	4.603667
284.427158	7281.165876	14.736231	-0.057882	4.601201
284.463990	7273.225474	14.741235	-0.057884	4.598772
284.521976	7265.177104	14.746240	-0.057890	4.596308
284.525170	7257.139145	14.751245	-0.057885	4.593847
284.434512	7249.111626	14.756250	-0.057863	4.591387
284.238744	7241.099685	14.761255	-0.057821	4.588930
284.404797	7233.126525	14.766259	-0.057847	4.586485
284.394859	7225.112942	14.771264	-0.057840	4.584025
284.282035	7217.093602	14.776269	-0.057814	4.581562
284.262989	7209.137441	14.781274	-0.057806	4.579118
284.077898	7201.144133	14.786279	-0.057766	4.576661
284.051139	7193.123505	14.791283	-0.057756	4.574194
284.027844	7185.131558	14.796288	-0.057746	4.571734
284.074848	7177.099195	14.801293	-0.057750	4.569261
284.039835	7169.176705	14.806298	-0.057738	4.566820
283.823523	7161.083714	14.811303	-0.057693	4.564325
283.882154	7153.187851	14.816307	-0.057699	4.561890
283.681419	7145.187645	14.821312	-0.057656	4.559421
283.801309	7137.184876	14.826317	-0.057673	4.556950
283.864098	7129.134044	14.831322	-0.057680	4.554463
283.727659	7121.117526	14.836327	-0.057649	4.551986
283.627738	7113.094208	14.841331	-0.057626	4.549504
283.583845	7105.148745	14.846336	-0.057612	4.547046
283.629184	7097.098382	14.851341	-0.057616	4.544553
283.593010	7089.155529	14.856346	-0.057604	4.542093
283.502762	7081.130625	14.861351	-0.057582	4.539606
283.435766	7073.139249	14.866355	-0.057564	4.537127
283.383788	7065.085812	14.871360	-0.057550	4.534628
283.318658	7057.085165	14.876365	-0.057532	4.532145
283.372888	7049.084320	14.881370	-0.057537	4.529659
283.075730	7041.080645	14.886375	-0.057477	4.527172
283.321025	7033.109678	14.891379	-0.057517	4.524693
283.167875	7025.189360	14.896384	-0.057484	4.522229
282.944928	7017.113415	14.901389	-0.057437	4.519714
283.032948	7009.181487	14.906394	-0.057448	4.517244
282.899139	7001.079981	14.911399	-0.057418	4.514719
283.128083	6993.049818	14.916403	-0.057456	4.512215
282.949507	6985.058722	14.921408	-0.057418	4.509722
282.943937	6977.039959	14.926413	-0.057411	4.507218
283.014602	6969.059104	14.931418	-0.057419	4.504726
282.924992	6961.068815	14.936423	-0.057398	4.502229
282.899677	6953.077538	14.941427	-0.057388	4.499730
282.850709	6945.114840	14.946432	-0.057374	4.497238
282.708932	6937.036659	14.951437	-0.057342	4.494709
282.688192	6929.100638	14.956442	-0.057333	4.492223
282.677682	6921.048435	14.961447	-0.057326	4.489700
282.603935	6913.062016	14.966451	-0.057307	4.487196
282.444166	6905.042031	14.971456	-0.057272	4.484679
282.533141	6897.039361	14.976461	-0.057284	4.482167
282.699490	6889.056359	14.981466	-0.057309	4.479660
282.462955	6881.120173	14.986471	-0.057260	4.477165
282.391925	6873.046026	14.991475	-0.057242	4.474626
282.546777	6865.031887	14.996480	-0.057266	4.472105
282.436737	6857.017845	15.001485	-0.057240	4.469582
282.423060	6849.054988	15.006490	-0.057232	4.467074
282.554535	6840.998100	15.011495	-0.057252	4.464535
282.396029	6833.111055	15.016499	-0.057217	4.462047
282.301917	6825.029964	15.021504	-0.057194	4.459497
282.127211	6817.033491	15.026509	-0.057157	4.456972
282.104672	6809.049854	15.031514	-0.057148	4.454450
282.055562	6800.978224	15.036519	-0.057133	4.451899
282.075854	6793.018042	15.041523	-0.057132	4.449382
281.959225	6785.030399	15.046528	-0.057105	4.446854
282.015684	6777.013787	15.051533	-0.057110	4.444316
282.022396	6769.033858	15.056538	-0.057107	4.441788
281.796334	6761.016971	15.061543	-0.057059	4.439246
281.980218	6753.039119	15.066547	-0.057088	4.436716
281.599148	6744.990161	15.071552	-0.057012	4.434161
281.449020	6736.954882	15.076557	-0.056979	4.431609
281.586495	6728.957940	15.081562	-0.057000	4.429069
281.495892	6720.959673	15.086567	-0.056978	4.426526
281.511647	6712.978378	15.091571	-0.056976	4.423987
281.401437	6705.027874	15.096576	-0.056950	4.421457
281.397739	6696.998191	15.101581	-0.056944	4.418900
281.329378	6689.029894	15.106586	-0.056926	4.416361
281.213863	6680.948415	15.111591	-0.056900	4.413784
281.397977	6672.949644	15.116595	-0.056929	4.411233
281.262888	6664.981542	15.121600	-0.056899	4.408689
281.026103	6656.952150	15.126605	-0.056849	4.406124
281.183924	6649.002772	15.131610	-0.056874	4.403585
280.933001	6640.978144	15.136615	-0.056822	4.401018
280.753027	6633.019668	15.141619	-0.056783	4.398471
280.786224	6625.009954	15.146624	-0.056784	4.395907
281.005550	6616.965954	15.151629	-0.056820	4.393332
280.896223	6608.927877	15.156634	-0.056794	4.390755
280.834940	6600.965827	15.161639	-0.056778	4.388201
281.063063	6592.960970	15.166643	-0.056815	4.385634
280.760623	6584.991749	15.171648	-0.056754	4.383074
280.490618	6576.977226	15.176653	-0.056698	4.380498
280.651121	6569.047719	15.181658	-0.056723	4.377950
280.569747	6560.964802	15.186663	-0.056703	4.375350
280.531297	6552.983952	15.191667	-0.056691	4.372782
280.533712	6544.974150	15.196672	-0.056686	4.370203
280.682228	6536.981055	15.201677	-0.056708	4.367628
280.642837	6528.992077	15.206682	-0.056696	4.365053
280.358481	6520.983198	15.211687	-0.056638	4.362468
280.509595	6513.004182	15.216691	-0.056661	4.359893
280.511871	6505.086670	15.221696	-0.056656	4.357336
280.205512	6496.949647	15.226701	-0.056594	4.354705
280.433381	6488.867533	15.231706	-0.056631	4.352093
280.473614	6480.861261	15.236711	-0.056634	4.349503
280.249411	6472.971813	15.241715	-0.056587	4.346948
280.274426	6464.957035	15.246720	-0.056586	4.344352
280.152000	6456.956658	15.251725	-0.056559	4.341758
280.386099	6449.003189	15.256730	-0.056597	4.339180
280.091198	6440.953296	15.261735	-0.056537	4.336566
280.038122	6432.959285	15.266739	-0.056522	4.333970
280.040745	6424.957436	15.271744	-0.056517	4.331371
279.907439	6416.951658	15.276749	-0.056487	4.328767
280.053913	6408.958414	15.281754	-0.056510	4.326168
279.852837	6400.981001	15.286759	-0.056467	4.323570
279.737209	6392.969299	15.291763	-0.056440	4.320960
279.688081	6384.985024	15.296768	-0.056426	4.318358
279.777158	6376.968170	15.301773	-0.056438	4.315745
279.759072	6368.924980	15.306778	-0.056429	4.313120
279.435967	6360.901960	15.311783	-0.056364	4.310499
279.516978	6352.959141	15.316787	-0.056374	4.307905
279.507963	6344.906589	15.321792	-0.056367	4.305273
279.519193	6336.915775	15.326797	-0.056364	4.302659
279.446259	6328.944119	15.331802	-0.056345	4.300050
279.428488	6320.937958	15.336807	-0.056337	4.297428
279.365445	6312.954883	15.341811	-0.056320	4.294812
279.080823	6304.939959	15.346816	-0.056262	4.292182
279.324770	6296.874902	15.351821	-0.056302	4.289538
279.243137	6288.926035	15.356826	-0.056282	4.286928
279.116118	6280.905214	15.361831	-0.056253	4.284292
278.956846	6272.952833	15.366835	-0.056218	4.281677
278.946822	6264.911622	15.371840	-0.056211	4.279033
278.791010	6256.943437	15.376845	-0.056177	4.276409
278.919765	6248.922990	15.381850	-0.056196	4.273769
278.715451	6240.874967	15.386855	-0.056153	4.271116
278.747427	6232.899980	15.391859	-0.056154	4.268487
278.677516	6224.887998	15.396864	-0.056135	4.265843
278.616963	6216.904418	15.401869	-0.056119	4.263207
278.744817	6208.879423	15.406874	-0.056138	4.260557
278.382934	6200.924856	15.411879	-0.056065	4.257925
278.685292	6192.908128	15.416883	-0.056116	4.255277
278.590674	6184.926449	15.421888	-0.056094	4.252634
278.364073	6176.839203	15.426893	-0.056046	4.249955
278.233133	6168.958080	15.431898	-0.056017	4.247342
278.260705	6160.871479	15.436903	-0.056017	4.244661
278.265432	6152.964637	15.441907	-0.056013	4.242038
278.181940	6144.895851	15.446912	-0.055992	4.239359
278.134054	6136.945864	15.451917	-0.055978	4.236718
278.112353	6128.902487	15.456922	-0.055969	4.234044
278.045103	6120.901127	15.461927	-0.055951	4.231382
277.935581	6112.874131	15.466931	-0.055926	4.228710
277.996090	6104.913092	15.471936	-0.055932	4.226059
278.043665	6096.919932	15.476941	-0.055935	4.223396
278.093512	6088.973859	15.481946	-0.055940	4.220747
278.240406	6080.920535	15.486951	-0.055962	4.218061
278.042290	6072.972919	15.491955	-0.055920	4.215406
277.686502	6064.946226	15.496960	-0.055848	4.212721
277.942905	6056.885430	15.501965	-0.055891	4.210029
277.835818	6048.956088	15.506970	-0.055866	4.207376
277.779021	6040.917484	15.511975	-0.055850	4.204685
277.722629	6032.994935	15.516979	-0.055835	4.202031
277.835582	6024.945687	15.521984	-0.055851	4.199334
277.566139	6016.980132	15.526989	-0.055795	4.196660
277.688959	6008.911117	15.531994	-0.055813	4.193954
277.540939	6000.797930	15.536999	-0.055780	4.191228
277.445816	5992.840793	15.542003	-0.055758	4.188553
277.181291	5984.855049	15.547008	-0.055703	4.185865
277.124682	5976.934856	15.552013	-0.055688	4.183200
277.318695	5968.884867	15.557018	-0.055719	4.180492
277.253594	5960.898234	15.562023	-0.055701	4.177801
277.305433	5952.876957	15.567027	-0.055706	4.175098
277.059799	5944.912935	15.572032	-0.055655	4.172409
277.023211	5936.893800	15.577037	-0.055643	4.169702
277.065628	5928.937403	15.582042	-0.055646	4.167015
277.004429	5920.906389	15.587047	-0.055629	4.164300
277.133442	5912.916866	15.592051	-0.055648	4.161599
276.952091	5904.939943	15.597056	-0.055609	4.158898
276.933029	5896.876272	15.602061	-0.055601	4.156167
277.095858	5888.888298	15.607066	-0.055626	4.153462
276.856485	5880.864649	15.612071	-0.055576	4.150739
276.848780	5872.864314	15.617075	-0.055570	4.148024
276.854847	5864.881629	15.622080	-0.055566	4.145314
276.816827	5856.897406	15.627085	-0.055553	4.142601
276.706480	5848.881443	15.632090	-0.055528	4.139875
276.519051	5840.912006	15.637095	-0.055488	4.137161
276.490969	5832.910263	15.642099	-0.055477	4.134437
276.366475	5824.849380	15.647104	-0.055449	4.131690
276.283047	5816.851989	15.652109	-0.055428	4.128963
276.406344	5808.893802	15.657114	-0.055446	4.126250
276.434441	5800.896636	15.662119	-0.055446	4.123520
276.217612	5792.891570	15.667123	-0.055401	4.120784
276.322368	5784.946128	15.672128	-0.055415	4.118069
276.262670	5776.890451	15.677133	-0.055399	4.115313
276.255525	5768.894837	15.682138	-0.055393	4.112577
276.123932	5760.826162	15.687143	-0.055363	4.109812
276.178322	5752.854518	15.692147	-0.055368	4.107081
276.155549	5744.855510	15.697152	-0.055359	4.104338
275.784890	5736.878395	15.702157	-0.055284	4.101596
275.962743	5728.924519	15.707162	-0.055312	4.098867
275.668206	5720.905457	15.712167	-0.055252	4.096108
275.686389	5712.889236	15.717171	-0.055251	4.093351
275.742242	5704.888779	15.722176	-0.055256	4.090599
275.650623	5696.933743	15.727181	-0.055234	4.087859
275.508219	5688.907221	15.732186	-0.055202	4.085092
275.531626	5680.910612	15.737191	-0.055201	4.082335
275.615270	5672.889033	15.742195	-0.055212	4.079569
275.508329	5664.977894	15.747200	-0.055187	4.076836
275.471474	5656.907674	15.752205	-0.055175	4.074047
275.706545	5648.916298	15.757210	-0.055213	4.071288
275.652702	5640.931708	15.762215	-0.055198	4.068525
275.473833	5632.949408	15.767219	-0.055160	4.065759
275.103305	5624.964930	15.772224	-0.055086	4.062988
275.098356	5616.918329	15.777229	-0.055080	4.060199
275.232760	5608.945442	15.782234	-0.055100	4.057435
274.834912	5600.899632	15.787239	-0.055020	4.054636
275.014951	5592.912473	15.792243	-0.055049	4.051864
274.892996	5584.949306	15.797248	-0.055021	4.049094
274.764680	5576.917441	15.802253	-0.054992	4.046298
274.754898	5568.941896	15.807258	-0.054985	4.043522
274.692148	5560.949840	15.812263	-0.054968	4.040737
274.760222	5552.960579	15.817267	-0.054976	4.037953
274.836301	5544.929947	15.822272	-0.054985	4.035153
274.721565	5536.805576	15.827277	-0.054958	4.032316
274.650695	5528.828084	15.832282	-0.054940	4.029528
274.449017	5520.880435	15.837287	-0.054897	4.026747
274.489523	5512.886137	15.842291	-0.054900	4.023951
274.458742	5504.921827	15.847296	-0.054889	4.021163
274.202463	5496.937991	15.852301	-0.054836	4.018362
274.351948	5488.922756	15.857306	-0.054859	4.015555
274.348607	5480.858297	15.862311	-0.054853	4.012726
274.316251	5472.872813	15.867315	-0.054842	4.009923
274.249727	5464.933519	15.872320	-0.054824	4.007133
274.193958	5456.907869	15.877325	-0.054809	4.004311
274.337898	5448.950081	15.882330	-0.054831	4.001514
274.205434	5440.950640	15.887335	-0.054801	3.998696
274.113626	5432.922311	15.892339	-0.054779	3.995867
274.191839	5424.925764	15.897344	-0.054788	3.993049
274.138123	5416.882362	15.902349	-0.054773	3.990211
274.070356	5408.924030	15.907354	-0.054755	3.987400
274.086425	5400.875671	15.912359	-0.054753	3.984557
273.996476	5392.959704	15.917363	-0.054731	3.981758
273.905131	5384.948842	15.922368	-0.054709	3.978922
273.895512	5376.926767	15.927373	-0.054702	3.976082
273.795681	5368.937491	15.932378	-0.054678	3.973250
273.672358	5360.901349	15.937383	-0.054650	3.970399
273.764729	5352.931398	15.942387	-0.054662	3.967573
273.788603	5344.906116	15.947392	-0.054662	3.964724
273.707043	5336.966201	15.952397	-0.054641	3.961902
273.475510	5328.985489	15.957402	-0.054593	3.959061
273.461132	5320.990713	15.962407	-0.054585	3.956216
273.576658	5312.977136	15.967411	-0.054602	3.953365
273.410666	5304.931020	15.972416	-0.054566	3.950495
273.309229	5296.921878	15.977421	-0.054542	3.947637
273.523409	5288.933176	15.982426	-0.054577	3.944790
273.270147	5280.977923	15.987431	-0.054524	3.941945
273.289626	5272.950707	15.992435	-0.054523	3.939077
273.477502	5264.970029	15.997440	-0.054553	3.936226
273.489327	5256.951319	16.002445	-0.054550	3.933357
273.405593	5248.944013	16.007450	-0.054529	3.930488
273.189495	5240.999609	16.012455	-0.054484	3.927637
273.222419	5232.955675	16.017459	-0.054485	3.924752
273.076513	5225.054327	16.022464	-0.054452	3.921914
272.790370	5216.979804	16.027469	-0.054394	3.919008
273.114693	5209.019830	16.032474	-0.054449	3.916153
272.868773	5200.995211	16.037479	-0.054398	3.913262
272.642474	5192.926230	16.042483	-0.054351	3.910353
272.821318	5184.996225	16.047488	-0.054379	3.907500
272.882221	5176.937685	16.052493	-0.054385	3.904596
272.729412	5169.047382	16.057498	-0.054352	3.901746
272.649329	5160.992370	16.062503	-0.054332	3.898837
272.678761	5152.995664	16.067507	-0.054332	3.895948
272.574568	5144.995367	16.072512	-0.054308	3.893053
272.384155	5136.950332	16.077517	-0.054267	3.890138
272.496743	5128.990490	16.082522	-0.054283	3.887258
272.352169	5120.985314	16.087527	-0.054251	3.884354
272.187347	5113.024253	16.092531	-0.054215	3.881464
272.349285	5105.058932	16.097536	-0.054240	3.878576
272.038959	5097.029839	16.102541	-0.054177	3.875654
271.989771	5088.823141	16.107546	-0.054163	3.872670
271.974738	5080.798571	16.112551	-0.054155	3.869750
271.900269	5072.861246	16.117555	-0.054136	3.866859
271.769566	5064.920051	16.122560	-0.054107	3.863964
271.765519	5056.930143	16.127565	-0.054101	3.861051
271.863628	5048.974986	16.132570	-0.054114	3.858150
271.660701	5040.965121	16.137575	-0.054071	3.855221
271.612181	5032.971853	16.142579	-0.054057	3.852299
271.643292	5024.974368	16.147584	-0.054057	3.849375
271.597807	5016.959851	16.152589	-0.054044	3.846441
271.911694	5008.994828	16.157594	-0.054097	3.843530
271.589386	5001.013664	16.162599	-0.054032	3.840598
271.591589	4993.034436	16.167603	-0.054027	3.837672
271.591315	4985.036786	16.172608	-0.054022	3.834736
271.350660	4977.005115	16.177613	-0.053972	3.831780
271.326064	4969.025416	16.182618	-0.053963	3.828846
271.073447	4961.020514	16.187623	-0.053910	3.825895
271.194281	4953.047534	16.192627	-0.053928	3.822962
271.366364	4945.080280	16.197632	-0.053955	3.820029
271.137642	4937.074900	16.202637	-0.053907	3.817072
270.988551	4929.073001	16.207642	-0.053874	3.814115
271.287898	4921.025641	16.212647	-0.053925	3.811149
271.074231	4913.067776	16.217651	-0.053880	3.808203
271.016184	4905.064222	16.222656	-0.053864	3.805241
270.848000	4897.120472	16.227661	-0.053828	3.802296
271.102343	4889.094547	16.232666	-0.053870	3.799328
271.091924	4881.106119	16.237671	-0.053863	3.796365
270.950082	4873.039076	16.242675	-0.053831	3.793368
270.908688	4865.045720	16.247680	-0.053818	3.790399
270.830296	4857.054102	16.252685	-0.053799	3.787427
270.912845	4849.068575	16.257690	-0.053809	3.784458
270.561090	4841.109841	16.262695	-0.053738	3.781487
270.521719	4833.107227	16.267699	-0.053726	3.778505
270.526783	4825.096602	16.272704	-0.053722	3.775518
270.397639	4817.061837	16.277709	-0.053692	3.772517
270.347878	4809.063886	16.282714	-0.053678	3.769529
270.325914	4801.095688	16.287719	-0.053669	3.766550
270.387728	4793.083724	16.292723	-0.053675	3.763555
270.360246	4785.135186	16.297728	-0.053665	3.760578
270.303690	4777.147238	16.302733	-0.053649	3.757584
270.378546	4769.099453	16.307738	-0.053658	3.754569
270.395054	4761.104905	16.312743	-0.053656	3.751569
270.339634	4753.054664	16.317747	-0.053641	3.748544
270.267450	4745.085874	16.322752	-0.053622	3.745547
270.086040	4737.148463	16.327757	-0.053583	3.742558
270.005453	4729.117594	16.332762	-0.053563	3.739532
269.851049	4721.174032	16.337767	-0.053529	3.736536
269.734570	4713.136078	16.342771	-0.053502	3.733502
269.781036	4705.100362	16.347776	-0.053506	3.730471
269.604339	4697.148718	16.352781	-0.053468	3.727463
269.800616	4689.125730	16.357786	-0.053499	3.724435
269.515587	4681.204589	16.362791	-0.053441	3.721432
269.692540	4673.178438	16.367795	-0.053469	3.718397
269.765141	4665.198306	16.372800	-0.053477	3.715375
269.537201	4657.081585	16.377805	-0.053430	3.712292
269.573009	4649.089785	16.382810	-0.053431	3.709259
269.636835	4641.116689	16.387815	-0.053438	3.706232
269.593384	4633.149561	16.392819	-0.053425	3.703202
269.468287	4625.186018	16.397824	-0.053397	3.700169
269.590599	4617.150034	16.402829	-0.053414	3.697112
269.632623	4609.170870	16.407834	-0.053417	3.694072
269.536785	4601.163827	16.412839	-0.053394	3.691016
269.304150	4593.198512	16.417843	-0.053346	3.687969
269.453521	4585.208462	16.422848	-0.053368	3.684920
268.996984	4577.268643	16.427853	-0.053278	3.681873
269.167289	4569.240699	16.432858	-0.053305	3.678805
269.307067	4561.236869	16.437863	-0.053326	3.675743
269.016639	4553.219174	16.442867	-0.053266	3.672662
268.990341	4545.231544	16.447872	-0.053256	3.669597
269.187739	4537.225203	16.452877	-0.053288	3.666528
269.072128	4529.298278	16.457882	-0.053261	3.663478
268.874559	4521.254470	16.462887	-0.053219	3.660380
268.652825	4513.243506	16.467891	-0.053173	3.657290
268.766051	4505.220988	16.472896	-0.053189	3.654202
268.656170	4497.199181	16.477901	-0.053163	3.651106
268.782181	4489.228956	16.482906	-0.053182	3.648033
268.656999	4481.207263	16.487911	-0.053153	3.644932
268.825033	4473.274266	16.492915	-0.053180	3.641869
268.574743	4465.293277	16.497920	-0.053128	3.638775
268.482907	4457.272919	16.502925	-0.053106	3.635666
268.566232	4449.260355	16.507930	-0.053116	3.632563
268.453500	4441.199690	16.512935	-0.053090	3.629433
268.210849	4433.236967	16.517939	-0.053040	3.626335
268.190078	4425.301979	16.522944	-0.053031	3.623251
268.178571	4417.250352	16.527949	-0.053023	3.620120
268.230752	4409.295882	16.532954	-0.053028	3.617025
268.244423	4401.273985	16.537959	-0.053025	3.613900
268.072418	4393.261590	16.542963	-0.052988	3.610771
268.015577	4385.310530	16.547968	-0.052973	3.607667
267.986987	4377.289259	16.552973	-0.052962	3.604533
267.988930	4369.354255	16.557978	-0.052957	3.601431
267.799580	4361.372605	16.562983	-0.052917	3.598303
267.838904	4353.349123	16.567987	-0.052919	3.595162
267.965415	4345.340781	16.572992	-0.052938	3.592026
267.576992	4337.364113	16.577997	-0.052860	3.588886
267.404499	4329.364090	16.583002	-0.052823	3.585740
267.490501	4321.387604	16.588007	-0.052834	3.582608
267.398186	4313.376913	16.593011	-0.052812	3.579454
267.390896	4305.422694	16.598016	-0.052805	3.576322
267.153490	4297.368515	16.603021	-0.052756	3.573142
267.177250	4289.375514	16.608026	-0.052755	3.569990
267.131716	4281.419893	16.613031	-0.052741	3.566849
266.964375	4273.407504	16.618035	-0.052705	3.563678
267.106858	4265.401817	16.623040	-0.052727	3.560517
267.071144	4257.424891	16.628045	-0.052715	3.557358
267.112121	4249.400606	16.633050	-0.052717	3.554181
266.933529	4241.324076	16.638055	-0.052679	3.550973
266.938209	4233.348356	16.643059	-0.052675	3.547808
267.036800	4225.368100	16.648064	-0.052688	3.544641
266.868862	4217.428822	16.653069	-0.052652	3.541480
267.085547	4209.413234	16.658074	-0.052687	3.538297
266.958719	4201.405291	16.663079	-0.052658	3.535104
266.724386	4193.408765	16.668083	-0.052609	3.531909
266.847725	4185.408436	16.673088	-0.052627	3.528720
266.731859	4177.397308	16.678093	-0.052600	3.525517
266.673852	4169.464888	16.683098	-0.052585	3.522345
266.464843	4161.463690	16.688103	-0.052540	3.519137
266.417135	4153.477939	16.693107	-0.052526	3.515938
266.578371	4145.458715	16.698112	-0.052551	3.512729
266.385429	4137.440252	16.703117	-0.052510	3.509506
266.359488	4129.463136	16.708122	-0.052500	3.506302
266.212188	4121.518137	16.713127	-0.052468	3.503104
266.247020	4113.475748	16.718131	-0.052469	3.499869
266.102555	4105.581658	16.723136	-0.052437	3.496686
266.171320	4097.529740	16.728141	-0.052445	3.493443
266.353677	4089.494288	16.733146	-0.052474	3.490207
266.191063	4081.538523	16.738151	-0.052438	3.486989
266.118499	4073.558482	16.743155	-0.052420	3.483762
266.126197	4065.581170	16.748160	-0.052416	3.480535
265.926178	4057.593557	16.753165	-0.052374	3.477294
266.039634	4049.572797	16.758170	-0.052390	3.474047
265.894802	4041.558975	16.763175	-0.052358	3.470792
265.589225	4033.595353	16.768179	-0.052296	3.467548
265.708951	4025.572028	16.773184	-0.052313	3.464291
265.654045	4017.576899	16.778189	-0.052297	3.461037
265.629482	4009.617570	16.783194	-0.052288	3.457795
265.500511	4001.608170	16.788199	-0.052259	3.454526
265.271077	3993.619000	16.793203	-0.052211	3.451259
265.479869	3985.613241	16.798208	-0.052244	3.447997
265.343085	3977.575425	16.803213	-0.052214	3.444707
265.336263	3969.644764	16.808218	-0.052208	3.441462
265.538511	3961.659832	16.813223	-0.052240	3.438198
265.246713	3953.666624	16.818227	-0.052181	3.434912
265.365965	3945.673867	16.823232	-0.052198	3.431636
265.122051	3937.645153	16.828237	-0.052147	3.428331
265.037165	3929.675155	16.833242	-0.052126	3.425051
265.068839	3921.704112	16.838247	-0.052127	3.421772
265.095428	3913.688840	16.843251	-0.052127	3.418472
265.035224	3905.702776	16.848256	-0.052111	3.415177
264.913516	3897.699245	16.853261	-0.052083	3.411870
264.979547	3889.687363	16.858266	-0.052090	3.408563
265.012212	3881.725220	16.863271	-0.052091	3.405271
264.877727	3873.749122	16.868275	-0.052061	3.401965
264.893973	3865.777415	16.873280	-0.052059	3.398663
264.553288	3857.791878	16.878285	-0.051990	3.395340
264.713731	3849.692249	16.883290	-0.052015	3.391983
264.615448	3841.687450	16.888295	-0.051991	3.388654
264.604713	3833.714770	16.893299	-0.051984	3.385337
264.594566	3825.783590	16.898304	-0.051977	3.382035
264.376347	3817.801246	16.903309	-0.051932	3.378700
264.413992	3809.793410	16.908314	-0.051933	3.375361
264.317534	3801.798808	16.913319	-0.051910	3.372019
264.061520	3793.806248	16.918323	-0.051858	3.368669
264.307667	3785.816540	16.923328	-0.051898	3.365335
264.105781	3777.853286	16.928333	-0.051856	3.361993
264.119465	3769.872273	16.933338	-0.051853	3.358647
264.109884	3761.861785	16.938343	-0.051846	3.355285
263.963812	3753.827915	16.943347	-0.051814	3.351905
264.158641	3745.822006	16.948352	-0.051845	3.348545
263.930412	3737.847751	16.953357	-0.051797	3.345180
263.999183	3729.899035	16.958362	-0.051805	3.341833
263.946591	3721.893997	16.963367	-0.051790	3.338455
263.816390	3713.906754	16.968371	-0.051761	3.335078
263.890013	3705.904107	16.973376	-0.051769	3.331699
263.803122	3697.907995	16.978381	-0.051748	3.328312
263.737595	3689.915996	16.983386	-0.051731	3.324925
263.469826	3681.951283	16.988391	-0.051676	3.321539
263.384190	3673.956114	16.993395	-0.051655	3.318143
263.511917	3665.982074	16.998400	-0.051673	3.314760
263.266886	3657.943172	17.003405	-0.051623	3.311332
263.231125	3649.964675	17.008410	-0.051611	3.307935
263.428169	3641.939453	17.013415	-0.051642	3.304522
263.205549	3633.994627	17.018419	-0.051596	3.301125
263.169329	3626.042313	17.023424	-0.051584	3.297728
263.088809	3618.022577	17.028429	-0.051564	3.294297
262.993797	3610.026383	17.033434	-0.051541	3.290872
263.071776	3602.044269	17.038439	-0.051551	3.287456
263.099507	3594.024694	17.043443	-0.051551	3.284018
263.201725	3586.070810	17.048448	-0.051565	3.280608
262.953075	3578.115240	17.053453	-0.051513	3.277180
262.992004	3570.114692	17.058458	-0.051515	3.273740
262.956924	3562.076306	17.063463	-0.051504	3.270278
262.726233	3554.109726	17.068467	-0.051456	3.266835
262.467772	3546.142604	17.073472	-0.051402	3.263387
262.478684	3538.115534	17.078477	-0.051399	3.259920
262.551827	3530.152681	17.083482	-0.051408	3.256479
262.517093	3522.135235	17.088487	-0.051396	3.253007
262.443164	3514.111225	17.093491	-0.051377	3.249527
262.570533	3506.157276	17.098496	-0.051396	3.246082
262.368164	3498.182305	17.103501	-0.051353	3.242610
262.425009	3490.182832	17.108506	-0.051359	3.239135
262.432487	3482.208654	17.113511	-0.051355	3.235665
262.260733	3474.162163	17.118515	-0.051318	3.232152
262.369334	3466.173705	17.123520	-0.051333	3.228672
262.168598	3458.188882	17.128525	-0.051290	3.225178
262.275727	3450.239199	17.133530	-0.051305	3.221708
262.408952	3442.236417	17.138535	-0.051325	3.218211
262.069137	3434.249333	17.143539	-0.051256	3.214699
262.125689	3426.266137	17.148544	-0.051262	3.211200
261.989299	3418.265612	17.153549	-0.051231	3.207682
261.919480	3410.279759	17.158554	-0.051213	3.204170
261.873278	3402.335231	17.163559	-0.051200	3.200672
261.803443	3394.331505	17.168563	-0.051181	3.197144
261.668693	3386.326504	17.173568	-0.051151	3.193609
261.639663	3378.311247	17.178573	-0.051141	3.190070
261.721013	3370.338922	17.183578	-0.051151	3.186550
261.642162	3362.358848	17.188583	-0.051131	3.183016
261.594396	3354.352313	17.193587	-0.051117	3.179468
261.915816	3346.398346	17.198592	-0.051172	3.175955
261.526935	3338.402816	17.203597	-0.051094	3.172389
261.506165	3330.422645	17.208602	-0.051085	3.168842
261.584582	3322.420163	17.213607	-0.051095	3.165285
261.561390	3314.443416	17.218611	-0.051085	3.161731
261.617910	3306.477069	17.223616	-0.051091	3.158181
261.526318	3298.431902	17.228621	-0.051068	3.154586
261.585713	3290.422541	17.233626	-0.051074	3.151009
261.323788	3282.479896	17.238631	-0.051021	3.147444
261.088532	3274.492246	17.243635	-0.050972	3.143856
261.221835	3266.519712	17.248640	-0.050991	3.140287
261.049324	3258.547082	17.253645	-0.050954	3.136700
260.903996	3250.562956	17.258650	-0.050922	3.133105
260.979541	3242.519985	17.263655	-0.050931	3.129489
261.015416	3234.553886	17.268659	-0.050932	3.125902
261.077347	3226.590896	17.273664	-0.050939	3.122313
260.785439	3218.629040	17.278669	-0.050879	3.118705
260.913132	3210.612362	17.283674	-0.050898	3.115086
260.972356	3202.606881	17.288679	-0.050904	3.111466
260.661057	3194.623990	17.293683	-0.050841	3.107835
260.898667	3186.625671	17.298688	-0.050880	3.104217
260.686443	3178.674433	17.303693	-0.050835	3.100596
260.402593	3170.730811	17.308698	-0.050777	3.096971
260.341463	3162.725049	17.313703	-0.050761	3.093324
260.429290	3154.668679	17.318707	-0.050772	3.089656
260.576669	3146.708853	17.323712	-0.050794	3.086030
260.305163	3138.734138	17.328717	-0.050739	3.082374
260.170073	3130.788719	17.333722	-0.050709	3.078734
260.065237	3122.822466	17.338727	-0.050684	3.075081
260.084224	3114.688547	17.343731	-0.050682	3.071352
260.243212	3106.697813	17.348736	-0.050707	3.067691
260.212955	3098.741163	17.353741	-0.050696	3.064033
260.223518	3090.768865	17.358746	-0.050693	3.060365
260.087429	3082.846787	17.363751	-0.050663	3.056708
260.003524	3074.858589	17.368755	-0.050642	3.053020
260.000358	3066.856299	17.373760	-0.050636	3.049324
259.799836	3058.863005	17.378765	-0.050594	3.045618
259.673972	3050.908951	17.383770	-0.050565	3.041930
259.697291	3042.929758	17.388775	-0.050564	3.038233
259.593264	3034.934387	17.393779	-0.050540	3.034517
259.567313	3026.930065	17.398784	-0.050530	3.030797
259.612421	3018.945680	17.403789	-0.050533	3.027084
259.417392	3010.977180	17.408794	-0.050492	3.023363
259.211935	3003.023689	17.413799	-0.050448	3.019644
259.142225	2995.021895	17.418803	-0.050430	3.015904
259.257218	2987.010828	17.423808	-0.050447	3.012164
259.183265	2979.016037	17.428813	-0.050428	3.008418
259.264871	2971.022971	17.433818	-0.050438	3.004676
259.262831	2963.065869	17.438823	-0.050432	3.000942
259.135483	2955.109244	17.443827	-0.050403	2.997197
259.017761	2947.127133	17.448832	-0.050376	2.993436
259.089776	2939.074862	17.453837	-0.050385	2.989646
258.984790	2931.099067	17.458842	-0.050360	2.985879
258.885233	2923.151319	17.463847	-0.050336	2.982121
258.837847	2915.155991	17.468851	-0.050322	2.978338
258.704391	2907.200408	17.473856	-0.050293	2.974565
258.504144	2899.195615	17.478861	-0.050250	2.970760
258.563688	2891.226107	17.483866	-0.050256	2.966980
258.560925	2883.235951	17.488871	-0.050250	2.963183
258.513150	2875.247084	17.493875	-0.050236	2.959378
258.404844	2867.306425	17.498880	-0.050211	2.955589
258.285709	2859.301312	17.503885	-0.050184	2.951764
258.374316	2851.291503	17.508890	-0.050195	2.947942
258.250758	2843.329875	17.513895	-0.050167	2.944127
258.118016	2835.342493	17.518899	-0.050137	2.940295
258.276273	2827.380998	17.523904	-0.050162	2.936485
258.194801	2819.371238	17.528909	-0.050141	2.932634
258.143689	2811.399895	17.533914	-0.050127	2.928798
258.185042	2803.403060	17.538919	-0.050129	2.924950
257.990415	2795.461819	17.543923	-0.050088	2.921111
258.057517	2787.488372	17.548928	-0.050095	2.917265
257.998994	2779.448765	17.553933	-0.050079	2.913376
257.830083	2771.413310	17.558938	-0.050043	2.909478
257.647372	2763.480988	17.563943	-0.050004	2.905623
257.556983	2755.488727	17.568947	-0.049982	2.901739
257.747011	2747.521955	17.573952	-0.050012	2.897878
257.499436	2739.551085	17.578957	-0.049961	2.893986
257.338903	2731.562257	17.583962	-0.049926	2.890084
257.343808	2723.604375	17.588967	-0.049922	2.886201
257.283190	2715.617207	17.593971	-0.049905	2.882295
257.102330	2707.679745	17.598976	-0.049867	2.878402
257.473927	2699.633769	17.603981	-0.049931	2.874480
257.547901	2691.620901	17.608986	-0.049939	2.870553
257.329848	2683.688362	17.613991	-0.049894	2.866644
257.107021	2675.720367	17.618995	-0.049847	2.862712
257.175357	2667.753649	17.624000	-0.049855	2.858791
257.011313	2659.787199	17.629005	-0.049819	2.854852
256.982321	2651.776245	17.634010	-0.049808	2.850893
257.038487	2643.798386	17.639015	-0.049814	2.846949
256.989558	2635.802459	17.644019	-0.049800	2.842986
256.952787	2627.872938	17.649024	-0.049788	2.839050
256.736710	2619.907511	17.654029	-0.049742	2.835081
256.662464	2611.883981	17.659034	-0.049723	2.831085
256.653132	2603.899522	17.664039	-0.049716	2.827107
256.383375	2595.941527	17.669043	-0.049661	2.823122
256.660561	2587.930760	17.674048	-0.049708	2.819136
256.373291	2579.991192	17.679053	-0.049649	2.815148
256.511498	2571.972072	17.684058	-0.049670	2.811138
256.610440	2563.988709	17.689063	-0.049683	2.807138
256.463634	2556.029940	17.694067	-0.049651	2.803131
256.265943	2548.095917	17.699072	-0.049609	2.799128
256.229636	2540.108969	17.704077	-0.049597	2.795101
256.278088	2532.097197	17.709082	-0.049601	2.791062
256.162037	2524.138827	17.714087	-0.049574	2.787033
256.131681	2516.143281	17.719091	-0.049563	2.782985
256.205217	2508.187979	17.724096	-0.049572	2.778958
256.070046	2500.228426	17.729101	-0.049542	2.774910
256.016809	2492.228074	17.734106	-0.049526	2.770841
255.973567	2484.253663	17.739111	-0.049513	2.766779
255.822640	2476.282121	17.744115	-0.049480	2.762706
255.678881	2468.336246	17.749120	-0.049448	2.758641
255.630455	2460.338535	17.754125	-0.049434	2.754549
255.749603	2452.255724	17.759130	-0.049451	2.750418
255.530956	2444.320754	17.764135	-0.049405	2.746335
255.563699	2436.328666	17.769139	-0.049406	2.742233
255.850700	2428.365884	17.774144	-0.049455	2.738154
255.707311	2420.403796	17.779149	-0.049423	2.734044
255.348792	2412.438664	17.784154	-0.049351	2.729913
255.388509	2404.489981	17.789159	-0.049353	2.725809
255.359904	2396.517939	17.794163	-0.049343	2.721682
255.418734	2388.557854	17.799168	-0.049349	2.717560
255.145074	2380.584441	17.804173	-0.049293	2.713405
255.129947	2372.556592	17.809178	-0.049285	2.709230
255.129598	2364.602872	17.814183	-0.049280	2.705089
255.070218	2356.636077	17.819187	-0.049263	2.700932
255.182843	2348.672939	17.824192	-0.049279	2.696780
255.024649	2340.689458	17.829197	-0.049245	2.692594
254.984712	2332.706659	17.834202	-0.049232	2.688410
254.936564	2324.749187	17.839207	-0.049218	2.684232
254.791846	2316.792614	17.844211	-0.049186	2.680041
254.645231	2308.854129	17.849216	-0.049154	2.675854
254.611639	2300.839928	17.854221	-0.049142	2.671627
254.623747	2292.837621	17.859226	-0.049139	2.667403
254.639797	2284.876998	17.864231	-0.049137	2.663194
254.555604	2276.881048	17.869235	-0.049117	2.658953
254.747197	2268.916095	17.874240	-0.049147	2.654740
254.491680	2260.938894	17.879245	-0.049094	2.650485
254.394536	2252.990491	17.884250	-0.049071	2.646248
254.281312	2245.055372	17.889255	-0.049045	2.642011
254.156593	2237.066388	17.894259	-0.049017	2.637737
254.147435	2229.106874	17.899264	-0.049010	2.633480
254.022527	2221.096997	17.904269	-0.048982	2.629181
253.989118	2213.112581	17.909274	-0.048970	2.624895
254.024925	2205.173326	17.914279	-0.048972	2.620630
253.765604	2197.234999	17.919283	-0.048918	2.616340
253.922256	2189.215618	17.924288	-0.048942	2.612026
253.834302	2181.231293	17.929293	-0.048921	2.607708
253.831728	2173.277333	17.934298	-0.048915	2.603405
253.722562	2165.357816	17.939303	-0.048890	2.599107
253.817989	2157.353314	17.944307	-0.048903	2.594768
253.886613	2149.177290	17.949312	-0.048910	2.590328
253.678507	2141.262258	17.954317	-0.048866	2.586003
253.623105	2133.326352	17.959322	-0.048851	2.581670
253.753769	2125.381654	17.964327	-0.048870	2.577338
253.352689	2117.450775	17.969331	-0.048790	2.572969
253.519959	2109.474200	17.974336	-0.048817	2.568607
253.338727	2101.523367	17.979341	-0.048778	2.564228
253.306112	2093.581680	17.984346	-0.048767	2.559856
253.191008	2085.652091	17.989351	-0.048740	2.555478
253.053460	2077.653109	17.994355	-0.048709	2.551052
252.944551	2069.697740	17.999360	-0.048684	2.546645
253.030756	2061.708396	18.004365	-0.048695	2.542225
253.126616	2053.737285	18.009370	-0.048708	2.537808
253.092445	2045.776032	18.014375	-0.048696	2.533380
252.964745	2037.800292	18.019379	-0.048667	2.528929
253.000620	2029.834026	18.024384	-0.048669	2.524488
252.843040	2021.907010	18.029389	-0.048634	2.520046
252.808594	2013.949622	18.034394	-0.048623	2.515589
252.873045	2005.932788	18.039399	-0.048630	2.511097
252.795933	1997.942302	18.044403	-0.048610	2.506602
252.725511	1990.008833	18.049408	-0.048592	2.502132
252.522889	1982.068971	18.054413	-0.048549	2.497640
252.347914	1974.126697	18.059418	-0.048512	2.493141
252.546898	1966.101280	18.064423	-0.048544	2.488613
252.282729	1958.155690	18.069427	-0.048489	2.484089
252.376061	1950.203450	18.074432	-0.048502	2.479579
252.396847	1942.251720	18.079437	-0.048500	2.475056
252.121797	1934.278769	18.084442	-0.048444	2.470491
252.164893	1926.323053	18.089447	-0.048447	2.465950
252.091343	1918.347535	18.094451	-0.048428	2.461381
252.074810	1910.407180	18.099456	-0.048420	2.456828
251.897740	1902.449831	18.104461	-0.048382	2.452245
251.885033	1894.464012	18.109466	-0.048374	2.447649
252.167855	1886.482351	18.114471	-0.048422	2.443069
251.890427	1878.560064	18.119475	-0.048365	2.438473
251.811295	1870.600423	18.124480	-0.048345	2.433861
251.907608	1862.544599	18.129485	-0.048358	2.429198
251.571888	1854.622844	18.134490	-0.048291	2.424571
251.491482	1846.690233	18.139495	-0.048271	2.419948
251.399641	1838.731006	18.144499	-0.048248	2.415300
251.522404	1830.738197	18.149504	-0.048266	2.410640
251.412818	1822.796611	18.154509	-0.048241	2.405983
251.263729	1814.861613	18.159514	-0.048208	2.401318
251.234176	1806.928358	18.164519	-0.048197	2.396654
251.140898	1798.923158	18.169523	-0.048175	2.391933
251.276278	1790.955935	18.174528	-0.048195	2.387243
251.272713	1783.000394	18.179533	-0.048189	2.382541
251.196573	1775.053932	18.184538	-0.048170	2.377828
251.142582	1767.111889	18.189543	-0.048155	2.373111
251.141120	1759.124335	18.194547	-0.048149	2.368361
251.045226	1751.193218	18.199552	-0.048126	2.363627
250.886518	1743.266636	18.204557	-0.048092	2.358882
250.642855	1735.330784	18.209562	-0.048041	2.354115
250.854270	1727.301403	18.214567	-0.048076	2.349319
250.555386	1719.349394	18.219571	-0.048015	2.344518
250.489206	1711.424100	18.224576	-0.047997	2.339742
250.716989	1703.426343	18.229581	-0.048035	2.334937
250.746264	1695.459425	18.234586	-0.048035	2.330124
250.379711	1687.551886	18.239591	-0.047962	2.325305
250.162193	1679.601392	18.244595	-0.047916	2.320462
250.474311	1671.647793	18.249600	-0.047969	2.315651
250.288649	1663.682710	18.254605	-0.047930	2.310781
250.268935	1655.722841	18.259610	-0.047921	2.305918
250.306544	1647.777529	18.264615	-0.047923	2.301058
250.184324	1639.837806	18.269619	-0.047895	2.296179
250.089980	1631.898015	18.274624	-0.047872	2.291291
250.291096	1623.899441	18.279629	-0.047904	2.286381
250.199095	1615.971104	18.284634	-0.047882	2.281479
250.028549	1608.073450	18.289639	-0.047845	2.276579
249.885629	1600.044968	18.294643	-0.047814	2.271590
250.049273	1592.048828	18.299648	-0.047839	2.266636
249.792298	1584.136246	18.304653	-0.047786	2.261687
249.607980	1576.213841	18.309658	-0.047747	2.256727
249.914835	1568.229606	18.314663	-0.047799	2.251760
249.588959	1560.302152	18.319667	-0.047733	2.246763
249.561386	1552.379593	18.324672	-0.047723	2.241784
249.460201	1544.447995	18.329677	-0.047699	2.236781
249.635671	1536.448899	18.334682	-0.047726	2.231749
249.592242	1528.505437	18.339687	-0.047713	2.226722
249.378107	1520.576505	18.344691	-0.047668	2.221677
249.498580	1512.631607	18.349696	-0.047686	2.216640
249.331433	1504.683553	18.354701	-0.047650	2.211564
249.354352	1496.728859	18.359706	-0.047649	2.206489
249.334458	1488.812837	18.364711	-0.047640	2.201424
249.212029	1480.880355	18.369715	-0.047612	2.196327
249.140959	1472.915202	18.374720	-0.047594	2.191201
249.178500	1464.936920	18.379725	-0.047596	2.186065
249.111844	1457.005604	18.384730	-0.047578	2.180938
249.086269	1449.088356	18.389735	-0.047568	2.175811
248.799685	1441.147478	18.394739	-0.047510	2.170633
248.987065	1433.188635	18.399744	-0.047540	2.165475
248.712248	1425.291372	18.404749	-0.047483	2.160302
248.360949	1417.381866	18.409754	-0.047413	2.155101
248.543316	1409.388217	18.414759	-0.047442	2.149882
248.480503	1401.429129	18.419763	-0.047425	2.144650
248.456005	1393.526411	18.424768	-0.047415	2.139446
248.434956	1385.581226	18.429773	-0.047406	2.134202
248.502929	1377.598491	18.434778	-0.047414	2.128928
248.444125	1369.683998	18.439783	-0.047398	2.123675
248.332511	1361.768091	18.444787	-0.047372	2.118402
248.255738	1353.822957	18.449792	-0.047353	2.113100
248.258643	1345.822841	18.454797	-0.047348	2.107756
248.104410	1337.905246	18.459802	-0.047314	2.102438
248.227372	1329.975374	18.464807	-0.047332	2.097125
248.020311	1322.053498	18.469811	-0.047288	2.091772
247.798072	1314.149616	18.474816	-0.047242	2.086416
247.748409	1306.228231	18.479821	-0.047228	2.081051
247.574428	1298.309044	18.484826	-0.047190	2.075662
247.774196	1290.321315	18.489831	-0.047222	2.070248
247.478168	1282.406651	18.494835	-0.047162	2.064822
247.477813	1274.491979	18.499840	-0.047157	2.059410
247.536928	1266.555063	18.504845	-0.047163	2.053975
247.278090	1258.628672	18.509850	-0.047110	2.048500
247.249715	1250.717936	18.514855	-0.047099	2.043045
247.230438	1242.783005	18.519859	-0.047091	2.037560
247.336534	1234.828974	18.524864	-0.047105	2.032059
247.178249	1226.886565	18.529869	-0.047071	2.026524
247.079248	1218.974452	18.534874	-0.047047	2.021001
246.981188	1211.085888	18.539879	-0.047024	2.015480
246.851573	1203.125521	18.544883	-0.046995	2.009890
246.799316	1195.211889	18.549888	-0.046980	2.004325
246.810755	1187.296217	18.554893	-0.046977	1.998750
246.805804	1179.354935	18.559898	-0.046971	1.993140
246.750241	1171.435360	18.564903	-0.046956	1.987523
246.596772	1163.516313	18.569907	-0.046922	1.981881
246.645771	1155.602916	18.574912	-0.046926	1.976248
246.507380	1147.679937	18.579917	-0.046895	1.970572
246.372231	1139.759156	18.584922	-0.046865	1.964882
246.611437	1131.836066	18.589927	-0.046904	1.959214
246.401509	1123.917645	18.594931	-0.046860	1.953484
246.224390	1115.981892	18.599936	-0.046822	1.947728
246.023739	1108.085066	18.604941	-0.046780	1.941981
245.964460	1100.164161	18.609946	-0.046764	1.936215
246.052228	1092.229591	18.614951	-0.046775	1.930437
246.056559	1084.293729	18.619955	-0.046771	1.924632
246.156252	1076.395015	18.624960	-0.046784	1.918848
245.900943	1068.508138	18.629965	-0.046732	1.913015
245.927488	1060.565326	18.634970	-0.046731	1.907154
245.804331	1052.676258	18.639975	-0.046703	1.901299
245.760744	1044.770554	18.644979	-0.046690	1.895422
245.738672	1036.855570	18.649984	-0.046681	1.889522
245.701465	1028.938605	18.654989	-0.046669	1.883600
245.613696	1021.051104	18.659994	-0.046648	1.877676
245.553215	1013.136930	18.664999	-0.046631	1.871716
245.419985	1005.221686	18.670003	-0.046601	1.865728
245.428980	997.322779	18.675008	-0.046598	1.859750
245.354735	989.426242	18.680013	-0.046579	1.853744
245.224703	981.510474	18.685018	-0.046550	1.847698
245.214072	973.620134	18.690023	-0.046543	1.841665
245.079521	965.737850	18.695027	-0.046513	1.835604
244.995300	957.832430	18.700032	-0.046492	1.829511
245.017254	949.921307	18.705037	-0.046491	1.823406
244.968796	942.022516	18.710042	-0.046477	1.817281
244.738530	934.158940	18.715047	-0.046429	1.811141
244.734873	926.237260	18.720051	-0.046423	1.804962
244.669401	918.379100	18.725056	-0.046406	1.798805
244.382850	910.488617	18.730061	-0.046348	1.792574
244.377625	902.528411	18.735066	-0.046342	1.786300
244.414549	894.644169	18.740071	-0.046344	1.780070
244.194789	886.780396	18.745075	-0.046298	1.773802
244.239536	878.861565	18.750080	-0.046301	1.767501
244.258966	870.983014	18.755085	-0.046299	1.761206
244.074286	863.119125	18.760090	-0.046260	1.754875
244.182269	855.202438	18.765095	-0.046275	1.748515
243.978575	847.336698	18.770099	-0.046232	1.742134
244.075278	839.446568	18.775104	-0.046245	1.735748
243.942138	831.572915	18.780109	-0.046215	1.729322
243.790621	823.702688	18.785114	-0.046182	1.722873
243.825037	815.838899	18.790119	-0.046183	1.716429
243.584947	807.960090	18.795123	-0.046134	1.709912
243.567992	800.072591	18.800128	-0.046125	1.703393
243.474523	792.212099	18.805133	-0.046103	1.696860
243.419531	784.323824	18.810138	-0.046088	1.690285
243.197503	776.494130	18.815143	-0.046041	1.683710
243.286913	768.599494	18.820147	-0.046053	1.677097
243.395621	760.692483	18.825152	-0.046068	1.670449
243.215128	752.852331	18.830157	-0.046029	1.663793
243.069329	745.010102	18.835162	-0.045997	1.657113
243.199987	737.111967	18.840167	-0.046017	1.650395
242.864049	729.297320	18.845171	-0.045949	1.643658
242.782818	721.458096	18.850176	-0.045929	1.636907
242.753147	713.528609	18.855181	-0.045918	1.630057
242.704250	705.658125	18.860186	-0.045904	1.623227
242.635076	697.832225	18.865191	-0.045886	1.616404
242.333382	689.994300	18.870195	-0.045825	1.609509
242.429513	682.125366	18.875200	-0.045838	1.602612
242.448406	674.280270	18.880205	-0.045836	1.595697
242.357792	666.420044	18.885210	-0.045814	1.588721
242.216387	658.594653	18.890215	-0.045783	1.581739
241.839324	650.808216	18.895219	-0.045708	1.574727
241.865541	642.936403	18.900224	-0.045708	1.567665
241.915295	635.084405	18.905229	-0.045712	1.560593
241.847577	627.254015	18.910234	-0.045694	1.553490
241.651395	619.420489	18.915239	-0.045653	1.546333
241.631438	611.574877	18.920243	-0.045644	1.539158
241.762615	603.723124	18.925248	-0.045664	1.531966
241.732006	595.889561	18.930253	-0.045653	1.524733
241.497683	588.099540	18.935258	-0.045604	1.517475
241.700533	580.234339	18.940263	-0.045637	1.510178
241.535530	572.422205	18.945267	-0.045601	1.502840
241.421671	564.631210	18.950272	-0.045575	1.495493
241.210626	556.837101	18.955277	-0.045531	1.488092
241.075263	549.029719	18.960282	-0.045501	1.480653
241.126671	541.206429	18.965287	-0.045505	1.473190
240.886297	533.371339	18.970291	-0.045455	1.465632
240.806367	525.587312	18.975296	-0.045435	1.458110
240.720289	517.777991	18.980301	-0.045414	1.450522
240.695091	509.970287	18.985306	-0.045405	1.442907
240.758894	502.183504	18.990311	-0.045412	1.435286
240.699887	494.364600	18.995315	-0.045396	1.427572
240.379713	486.626947	19.000320	-0.045331	1.419855
240.431441	478.824392	19.005325	-0.045336	1.412091
240.432543	471.025066	19.010330	-0.045331	1.404280
240.381800	463.270183	19.015335	-0.045317	1.396461
240.027690	455.512476	19.020339	-0.045246	1.388544
240.079259	447.725573	19.025344	-0.045250	1.380620
240.131505	439.939915	19.030349	-0.045255	1.372653
239.669443	432.223986	19.035354	-0.045164	1.364622
239.613436	424.483610	19.040359	-0.045149	1.356588
239.570970	416.691845	19.045363	-0.045136	1.348456
239.415611	408.953688	19.050368	-0.045102	1.340310
239.281580	401.214626	19.055373	-0.045072	1.332117
239.287821	393.444057	19.060378	-0.045068	1.323865
239.378229	385.698208	19.065383	-0.045080	1.315603
238.990387	377.869951	19.070387	-0.045003	1.307113
239.132406	370.116651	19.075392	-0.045024	1.298746
238.976288	362.415659	19.080397	-0.044990	1.290327
238.581737	354.745255	19.085402	-0.044912	1.281841
238.889329	346.984559	19.090407	-0.044964	1.273331
238.747552	339.273090	19.095411	-0.044933	1.264733
238.491776	331.609640	19.100416	-0.044880	1.256109
238.378628	323.914653	19.105421	-0.044854	1.247416
238.285167	316.231363	19.110426	-0.044832	1.238680
238.202562	308.537708	19.115431	-0.044812	1.229872
237.856436	300.879343	19.120435	-0.044742	1.220989
237.836139	293.198316	19.125440	-0.044734	1.212079
237.741904	285.526707	19.130445	-0.044711	1.203100
237.387869	277.904721	19.135450	-0.044640	1.194059
237.283044	270.242172	19.140455	-0.044616	1.184951
237.025831	262.614892	19.145459	-0.044563	1.175784
236.817445	254.974344	19.150464	-0.044520	1.166539
236.437240	247.397018	19.155469	-0.044444	1.157261
236.240415	239.731985	19.160474	-0.044402	1.147839
236.019982	232.120096	19.165479	-0.044357	1.138399
235.341450	224.574575	19.170483	-0.044225	1.128865
235.001001	216.993038	19.175488	-0.044157	1.119278
234.785267	209.386358	19.180493	-0.044112	1.109602
234.269004	201.834121	19.185498	-0.044011	1.099845
233.910581	194.283243	19.190503	-0.043940	1.090037
233.671776	186.703334	19.195507	-0.043890	1.080129
233.142651	179.188218	19.200512	-0.043787	1.070149
232.637677	171.666721	19.205517	-0.043688	1.060071
232.108870	164.157809	19.210522	-0.043585	1.049908
232.041052	156.595785	19.215527	-0.043567	1.039681
231.405087	149.133975	19.220531	-0.043444	1.029355
231.102621	141.621393	19.225536	-0.043383	1.018934
230.775783	134.133235	19.230541	-0.043317	1.008433
230.312323	126.682034	19.235546	-0.043226	0.997841
230.033625	119.175054	19.240551	-0.043170	0.987100
229.496492	111.747401	19.245555	-0.043065	0.976291
229.163772	104.300507	19.250560	-0.042998	0.965385
228.428056	96.947551	19.255565	-0.042856	0.954388
228.034906	89.528015	19.260570	-0.042779	0.943253
227.776118	82.126127	19.265575	-0.042726	0.932047
227.237607	74.777589	19.270579	-0.042621	0.920711
226.650887	67.452728	19.275584	-0.042507	0.909257
226.185826	60.353983	19.280589	-0.042416	0.898046