Tue Mar 23 11:07:36 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.425892	0.037080	0.000000	0.000022	0.723037

0.559937	-0.001656	0.005005	-0.000004	0.723008
0.618189	-0.007330	0.010010	-0.000014	0.723018
0.630111	-0.014302	0.015014	-0.000017	0.723008
0.692476	-0.022658	0.020019	-0.000029	0.723014
0.868220	-0.054020	0.025024	-0.000061	0.723014
0.829088	-0.048961	0.030029	-0.000054	0.723011
0.668837	-0.017369	0.035034	-0.000025	0.723017
0.454069	0.017604	0.040038	0.000015	0.723011
0.452247	0.018845	0.045043	0.000016	0.723013
0.341316	0.038594	0.050048	0.000036	0.723013
0.422733	0.021200	0.055053	0.000021	0.723007
0.500287	0.010976	0.060058	0.000006	0.723015
0.448916	0.015509	0.065062	0.000016	0.723006
0.450505	0.018808	0.070067	0.000015	0.723013
0.615316	-0.077543	0.075072	-0.000015	0.722882
0.562490	-0.162452	0.080077	-0.000006	0.722697
0.567071	-0.160403	0.085082	-0.000007	0.722703
0.696492	-0.188052	0.090086	-0.000031	0.722694
0.837313	-0.209898	0.095091	-0.000057	0.722701
0.544456	-0.156967	0.100096	-0.000003	0.722702
0.643280	-0.195390	0.105101	-0.000021	0.722662
0.773088	-0.361467	0.110106	-0.000046	0.722381
0.664789	-0.347789	0.115110	-0.000026	0.722370
0.608143	-0.334086	0.120115	-0.000015	0.722378
0.536267	-0.323434	0.125120	-0.000002	0.722374
0.440409	-0.332475	0.130125	0.000016	0.722323
0.335374	-0.435506	0.135130	0.000035	0.722084
0.246084	-0.423262	0.140134	0.000052	0.722077
0.395741	-0.448354	0.145139	0.000024	0.722080
0.587116	-0.483574	0.150144	-0.000012	0.722078
0.540389	-0.602860	0.155149	-0.000003	0.721828
0.731403	-0.673554	0.160154	-0.000039	0.721756
0.461935	-0.630780	0.165158	0.000011	0.721746
0.509977	-0.647947	0.170163	0.000002	0.721729
0.633971	-0.814513	0.175168	-0.000021	0.721445
0.531198	-0.798555	0.180173	-0.000002	0.721441
0.402570	-0.772121	0.185178	0.000022	0.721448
0.423519	-0.889815	0.190182	0.000018	0.721224
0.351259	-0.923168	0.195187	0.000031	0.721133
0.278469	-0.912309	0.200192	0.000045	0.721129
0.204177	-0.959969	0.205197	0.000058	0.721010
0.359197	-1.047217	0.210202	0.000030	0.720893
0.347500	-1.049415	0.215206	0.000032	0.720885
0.233153	-1.110858	0.220211	0.000053	0.720724
0.377962	-1.225202	0.225216	0.000026	0.720550
0.357649	-1.225230	0.230221	0.000029	0.720543
0.278718	-1.320203	0.235226	0.000044	0.720328
0.054738	-1.331199	0.240230	0.000086	0.720228
0.138310	-1.346870	0.245235	0.000070	0.720227
0.095893	-1.501566	0.250240	0.000078	0.719907
-0.015461	-1.485182	0.255245	0.000098	0.719901
0.254018	-1.594383	0.260250	0.000048	0.719780
0.008889	-1.640924	0.265254	0.000094	0.719603
0.011211	-1.637179	0.270259	0.000093	0.719611
-0.147115	-1.773985	0.275264	0.000123	0.719286
-0.134377	-1.783968	0.280269	0.000120	0.719271
-0.083453	-1.879598	0.285274	0.000111	0.719101
-0.552260	-1.867198	0.290278	0.000198	0.718961
-0.251548	-1.947675	0.295283	0.000142	0.718908
-0.210162	-2.086042	0.300288	0.000134	0.718649
-0.209199	-2.091509	0.305293	0.000134	0.718639
-0.304259	-2.208770	0.310298	0.000151	0.718374
-0.641194	-2.158570	0.315302	0.000214	0.718355
-1.009365	-2.212249	0.320307	0.000282	0.718120
-2.362485	-2.018650	0.325312	0.000534	0.718027
-2.370978	-2.024878	0.330317	0.000536	0.718012
-3.005254	-2.061901	0.335322	0.000654	0.717715
-3.384491	-1.998194	0.340326	0.000724	0.717708
-3.480281	-1.979753	0.345331	0.000742	0.717711
-3.310476	-2.139814	0.350336	0.000710	0.717454
-4.369255	-1.986382	0.355341	0.000907	0.717385
-4.195179	-2.014777	0.360346	0.000875	0.717391
-4.227781	-2.060225	0.365350	0.000880	0.717289
-5.207454	-1.987298	0.370355	0.001063	0.717089
-4.690166	-2.078670	0.375360	0.000966	0.717091
-5.338826	-1.965556	0.380365	0.001087	0.717086
-5.129344	-2.073300	0.385370	0.001048	0.716947
-5.891844	-2.033593	0.390374	0.001190	0.716757
-6.026761	-2.007712	0.395379	0.001215	0.716761
-6.384601	-1.943903	0.400384	0.001281	0.716761
-6.221349	-1.978495	0.405389	0.001251	0.716750
-6.261878	-2.114197	0.410394	0.001258	0.716468
-7.012899	-1.990608	0.415398	0.001398	0.716448
-7.092949	-1.973474	0.420403	0.001413	0.716454
-6.267337	-2.117714	0.425408	0.001259	0.716459
-7.017444	-2.037435	0.430413	0.001398	0.716354
-7.986377	-1.971666	0.435418	0.001579	0.716143
-7.619811	-2.042307	0.440422	0.001510	0.716132
-8.001806	-1.973839	0.445427	0.001581	0.716133
-7.586024	-2.046432	0.450432	0.001504	0.716137
-7.732286	-2.031292	0.455437	0.001531	0.716115
-8.329442	-2.039336	0.460442	0.001642	0.715889
-8.442074	-2.022858	0.465446	0.001663	0.715882
-8.672304	-1.978073	0.470451	0.001705	0.715890
-8.440431	-2.019684	0.475456	0.001662	0.715889
-8.881284	-1.944631	0.480461	0.001744	0.715883
-8.885281	-2.030292	0.485466	0.001745	0.715712
-9.664141	-1.973083	0.490470	0.001890	0.715550
-9.365727	-2.024146	0.495475	0.001834	0.715554
-9.621230	-1.980999	0.500480	0.001881	0.715550
-9.768955	-1.957796	0.505485	0.001909	0.715544
-9.391807	-2.019301	0.510490	0.001838	0.715556
-9.430012	-2.087262	0.515494	0.001845	0.715408
-10.978800	-1.896932	0.520499	0.002134	0.715238
-9.940181	-2.082787	0.525504	0.001940	0.715237
-10.484928	-1.988789	0.530509	0.002041	0.715231
-10.585731	-1.967569	0.535514	0.002060	0.715238
-10.102863	-2.056445	0.540518	0.001970	0.715232
-10.442634	-2.032468	0.545523	0.002033	0.715160
-11.369148	-1.989348	0.550528	0.002206	0.714918
-11.289524	-2.008405	0.555533	0.002191	0.714909
-11.623132	-1.943243	0.560538	0.002253	0.714920
-11.484651	-1.970306	0.565542	0.002227	0.714916
-11.263552	-2.009883	0.570547	0.002185	0.714916
-11.264101	-2.009313	0.575552	0.002185	0.714917
-11.615041	-2.031759	0.580557	0.002251	0.714748
-12.481402	-1.941430	0.585562	0.002412	0.714621
-11.927600	-2.044710	0.590566	0.002309	0.714613
-12.205314	-1.994575	0.595571	0.002360	0.714614
-12.345171	-1.967344	0.600576	0.002386	0.714619
-12.228335	-1.992791	0.605581	0.002364	0.714610
-11.881055	-2.051111	0.610586	0.002300	0.714617
-12.693811	-2.060129	0.615590	0.002451	0.714312
-13.349514	-1.957749	0.620595	0.002573	0.714284
-13.031504	-2.013136	0.625600	0.002513	0.714286
-13.214030	-1.985298	0.630605	0.002547	0.714277
-13.456831	-1.936274	0.635610	0.002592	0.714289
-13.312678	-1.967057	0.640614	0.002565	0.714279
-13.138724	-1.996235	0.645619	0.002533	0.714283
-13.259525	-2.085865	0.650624	0.002555	0.714062
-14.527654	-1.906544	0.655629	0.002791	0.713970
-14.103990	-1.977848	0.660634	0.002712	0.713978
-14.226817	-1.960248	0.665638	0.002735	0.713970
-14.522519	-1.907261	0.670643	0.002790	0.713971
-13.917395	-2.012380	0.675648	0.002677	0.713976
-14.301635	-1.948215	0.680653	0.002748	0.713968
-14.337064	-1.982028	0.685658	0.002755	0.713889
-14.986850	-1.984349	0.690662	0.002876	0.713654
-14.453234	-2.079245	0.695667	0.002776	0.713655
-15.309560	-1.924822	0.700672	0.002936	0.713659
-15.424370	-1.907196	0.705677	0.002957	0.713653
-14.979012	-1.982682	0.710682	0.002874	0.713661
-15.352586	-1.920296	0.715686	0.002943	0.713653
-15.557949	-1.883517	0.720691	0.002981	0.713654
-15.403115	-2.032930	0.725696	0.002952	0.713412
-16.228185	-1.912239	0.730701	0.003106	0.713360
-15.996559	-1.948675	0.735706	0.003063	0.713369
-15.776364	-1.993155	0.740710	0.003022	0.713359
-16.060728	-1.938420	0.745715	0.003074	0.713368
-16.065849	-1.937664	0.750720	0.003075	0.713367
-16.022672	-1.949670	0.755725	0.003067	0.713359
-16.011031	-2.060701	0.760730	0.003065	0.713143
-17.224260	-1.903982	0.765734	0.003291	0.713024
-17.177179	-1.911349	0.770739	0.003282	0.713027
-16.677947	-1.996361	0.775744	0.003189	0.713035
-17.045301	-1.937194	0.780749	0.003257	0.713023
-17.331398	-1.881523	0.785754	0.003310	0.713032
-17.105160	-1.926020	0.790758	0.003268	0.713024
-16.995546	-1.960680	0.795763	0.003247	0.712994
-17.624406	-1.989219	0.800768	0.003364	0.712714
-18.157761	-1.898476	0.805773	0.003463	0.712706
-18.088743	-1.906578	0.810778	0.003450	0.712715
-17.788013	-1.963208	0.815782	0.003394	0.712709
-18.065810	-1.914582	0.820787	0.003446	0.712707
-17.825849	-1.954194	0.825792	0.003401	0.712714
-17.699899	-1.982588	0.830797	0.003378	0.712702
-18.186071	-2.005966	0.835802	0.003468	0.712483
-19.150211	-1.880902	0.840806	0.003647	0.712391
-18.659736	-1.969807	0.845811	0.003556	0.712388
-18.750332	-1.951121	0.850816	0.003573	0.712393
-19.019547	-1.908018	0.855821	0.003623	0.712384
-18.701994	-1.960123	0.860826	0.003563	0.712393
-18.741626	-1.956196	0.865830	0.003571	0.712387
-19.027495	-1.951723	0.870835	0.003624	0.712294
-19.701496	-1.932095	0.875840	0.003749	0.712095
-19.457930	-1.978972	0.880845	0.003704	0.712088
-20.095430	-1.860975	0.885850	0.003822	0.712097
-19.994032	-1.879940	0.890854	0.003803	0.712095
-19.643915	-1.944075	0.895859	0.003738	0.712092
-19.682585	-1.933427	0.900864	0.003745	0.712100
-20.047684	-1.872847	0.905869	0.003813	0.712091
-19.937980	-2.017466	0.910874	0.003792	0.711842
-20.660119	-1.928851	0.915878	0.003927	0.711762
-20.840676	-1.895744	0.920883	0.003960	0.711764
-20.441009	-1.965343	0.925888	0.003886	0.711768
-20.592771	-1.943393	0.930893	0.003914	0.711758
-20.448692	-1.964326	0.935898	0.003887	0.711768
-20.548893	-1.948588	0.940902	0.003905	0.711764
-21.100097	-1.973563	0.945907	0.004008	0.711518
-21.473988	-1.935782	0.950912	0.004077	0.711461
-21.824003	-1.878977	0.955917	0.004142	0.711450
-21.437504	-1.943142	0.960922	0.004070	0.711460
-21.456539	-1.941628	0.965926	0.004074	0.711456
-21.670980	-1.903736	0.970931	0.004113	0.711456
-21.503233	-1.929593	0.975936	0.004082	0.711464
-21.546529	-2.010979	0.980941	0.004090	0.711286
-22.490972	-1.912710	0.985946	0.004266	0.711147
-22.657050	-1.886601	0.990950	0.004297	0.711140
-22.398247	-1.931342	0.995955	0.004248	0.711143
-22.068643	-1.987289	1.000960	0.004187	0.711149
-22.396747	-1.933916	1.005965	0.004248	0.711139
-22.361990	-1.934517	1.010970	0.004241	0.711151
-22.315661	-2.008453	1.015974	0.004232	0.711020
-23.328392	-1.900293	1.020979	0.004421	0.710876
-23.023320	-1.953396	1.025984	0.004364	0.710878
-23.439817	-1.883450	1.030989	0.004441	0.710870
-23.197594	-1.922503	1.035994	0.004396	0.710878
-23.196015	-1.924464	1.040998	0.004396	0.710875
-23.289876	-1.909657	1.046003	0.004413	0.710872
-23.100182	-2.040174	1.051008	0.004378	0.710679
-24.257045	-1.908090	1.056013	0.004593	0.710531
-24.034490	-1.943759	1.061018	0.004551	0.710539
-24.119444	-1.931787	1.066022	0.004567	0.710533
-24.357048	-1.889101	1.071027	0.004611	0.710534
-23.940088	-1.962336	1.076032	0.004533	0.710536
-24.128542	-1.932314	1.081037	0.004568	0.710530
-24.218436	-2.014413	1.086042	0.004585	0.710334
-25.212581	-1.894607	1.091046	0.004770	0.710219
-25.213694	-1.895541	1.096051	0.004770	0.710217
-24.831694	-1.960559	1.101056	0.004699	0.710224
-25.438395	-1.856676	1.106061	0.004812	0.710216
-25.196653	-1.895142	1.111066	0.004767	0.710225
-25.019161	-1.930203	1.116070	0.004733	0.710218
-25.240754	-1.921409	1.121075	0.004775	0.710157
-25.772237	-1.956659	1.126080	0.004873	0.709898
-25.859488	-1.944352	1.131085	0.004889	0.709891
-25.927112	-1.927542	1.136090	0.004902	0.709901
-26.106921	-1.897689	1.141094	0.004935	0.709897
-26.241709	-1.874766	1.146099	0.004960	0.709895
-26.074473	-1.903393	1.151104	0.004929	0.709898
-26.025014	-1.916577	1.156109	0.004920	0.709889
-26.279313	-1.999291	1.161114	0.004967	0.709633
-26.845639	-1.917029	1.166118	0.005072	0.709596
-26.860584	-1.914366	1.171123	0.005075	0.709596
-26.640337	-1.951231	1.176128	0.005034	0.709601
-26.718228	-1.940746	1.181133	0.005048	0.709595
-26.553488	-1.967292	1.186138	0.005017	0.709601
-26.825119	-1.943000	1.191142	0.005068	0.709553
-28.004116	-1.876555	1.196147	0.005287	0.709266
-27.417489	-1.979564	1.201152	0.005178	0.709269
-27.707115	-1.930842	1.206157	0.005232	0.709263
-28.020822	-1.871356	1.211162	0.005290	0.709271
-27.578285	-1.952200	1.216166	0.005207	0.709267
-27.893080	-1.897160	1.221171	0.005266	0.709265
-27.672673	-1.933744	1.226176	0.005225	0.709271
-28.079573	-1.995267	1.231181	0.005300	0.709003
-28.542024	-1.932077	1.236186	0.005386	0.708964
-28.632912	-1.919117	1.241190	0.005403	0.708958
-28.515542	-1.940928	1.246195	0.005381	0.708957
-28.393371	-1.958216	1.251200	0.005358	0.708966
-28.982371	-1.857510	1.256205	0.005468	0.708957
-28.703425	-1.902890	1.261210	0.005416	0.708966
-28.686241	-2.031504	1.266214	0.005413	0.708715
-29.559310	-1.913561	1.271219	0.005575	0.708640
-29.581294	-1.906021	1.276224	0.005579	0.708647
-29.449405	-1.935951	1.281229	0.005554	0.708635
-29.381891	-1.941594	1.286234	0.005542	0.708648
-29.731033	-1.882651	1.291238	0.005606	0.708642
-29.953275	-1.842971	1.296243	0.005648	0.708642
-29.276546	-2.044891	1.301248	0.005522	0.708479
-30.433907	-1.901661	1.306253	0.005737	0.708353
-30.266445	-1.928427	1.311258	0.005706	0.708360
-30.175867	-1.948190	1.316262	0.005689	0.708352
-30.405936	-1.907465	1.321267	0.005731	0.708352
-30.325324	-1.918598	1.326272	0.005716	0.708359
-30.502841	-1.891249	1.331277	0.005749	0.708351
-30.518225	-2.019589	1.336282	0.005752	0.708088
-31.122418	-1.948391	1.341286	0.005864	0.708015
-31.456449	-1.889761	1.346291	0.005926	0.708014
-31.123055	-1.944892	1.351296	0.005864	0.708022
-31.393107	-1.902100	1.356301	0.005914	0.708012
-31.242270	-1.925244	1.361306	0.005886	0.708020
-30.967447	-1.976554	1.366310	0.005835	0.708015
-31.467555	-2.030472	1.371315	0.005928	0.707728
-32.165902	-1.915786	1.376320	0.006058	0.707709
-32.453789	-1.869930	1.381325	0.006111	0.707698
-31.898151	-1.965526	1.386330	0.006008	0.707706
-32.104344	-1.932166	1.391334	0.006046	0.707699
-32.516500	-1.859028	1.396339	0.006122	0.707699
-31.883183	-1.968895	1.401344	0.006004	0.707705
-32.339669	-2.022275	1.406349	0.006089	0.707435
-33.453850	-1.851285	1.411354	0.006297	0.707380
-33.359704	-1.869891	1.416358	0.006279	0.707376
-32.968792	-1.940995	1.421363	0.006206	0.707374
-33.012109	-1.929271	1.426368	0.006214	0.707382
-33.357585	-1.872642	1.431373	0.006278	0.707372
-33.067080	-1.920682	1.436378	0.006224	0.707380
-33.032614	-1.978224	1.441382	0.006218	0.707277
-34.193641	-1.868180	1.446387	0.006434	0.707083
-33.633268	-1.965560	1.451392	0.006329	0.707088
-34.032510	-1.897403	1.456397	0.006403	0.707082
-34.154480	-1.873024	1.461402	0.006426	0.707088
-34.036578	-1.895241	1.466406	0.006404	0.707085
-34.136856	-1.880053	1.471411	0.006422	0.707080
-34.100251	-1.889297	1.476416	0.006415	0.707075
-34.997512	-1.891768	1.481421	0.006582	0.706749
-34.566193	-1.965414	1.486426	0.006502	0.706756
-34.791859	-1.926246	1.491430	0.006544	0.706754
-34.966347	-1.896975	1.496435	0.006576	0.706751
-34.717672	-1.937332	1.501440	0.006530	0.706759
-34.446213	-1.990024	1.506445	0.006479	0.706750
-34.767473	-1.957359	1.511450	0.006539	0.706701
-35.636778	-1.929698	1.516454	0.006701	0.706446
-35.613151	-1.935929	1.521459	0.006696	0.706442
-35.312115	-1.984766	1.526464	0.006640	0.706452
-35.701596	-1.920323	1.531469	0.006712	0.706442
-35.676464	-1.922512	1.536474	0.006707	0.706447
-35.678904	-1.923165	1.541478	0.006708	0.706445
-35.969311	-1.909536	1.546483	0.006762	0.706368
-36.489304	-1.934129	1.551488	0.006858	0.706133
-36.502519	-1.933987	1.556493	0.006861	0.706129
-36.738955	-1.889015	1.561498	0.006905	0.706135
-36.555993	-1.921741	1.566502	0.006870	0.706135
-36.847098	-1.874284	1.571507	0.006925	0.706126
-36.631699	-1.908677	1.576512	0.006884	0.706134
-36.798967	-1.883873	1.581517	0.006915	0.706124
-37.003836	-1.957447	1.586522	0.006953	0.705903
-37.200343	-1.940388	1.591526	0.006990	0.705867
-37.584630	-1.875854	1.596531	0.007061	0.705860
-37.398496	-1.903249	1.601536	0.007026	0.705871
-37.489798	-1.891749	1.606541	0.007043	0.705862
-37.380720	-1.909911	1.611546	0.007023	0.705865
-37.355877	-1.928616	1.616550	0.007018	0.705836
-38.205366	-1.932931	1.621555	0.007176	0.705523
-37.791052	-2.003210	1.626560	0.007099	0.705531
-38.587305	-1.866526	1.631565	0.007247	0.705520
-38.534352	-1.872824	1.636570	0.007237	0.705527
-37.984833	-1.973599	1.641574	0.007135	0.705521
-38.243771	-1.926750	1.646579	0.007183	0.705523
-38.225253	-1.974990	1.651584	0.007179	0.705433
-39.306454	-1.892837	1.656589	0.007380	0.705210
-39.002309	-1.943909	1.661594	0.007324	0.705217
-39.166998	-1.915835	1.666598	0.007354	0.705215
-39.427645	-1.871936	1.671603	0.007403	0.705210
-38.906720	-1.960872	1.676608	0.007306	0.705218
-39.188766	-1.914593	1.681613	0.007358	0.705210
-39.123263	-1.976535	1.686618	0.007346	0.705109
-39.650219	-1.990751	1.691622	0.007444	0.704891
-39.913075	-1.946418	1.696627	0.007492	0.704887
-40.148291	-1.901046	1.701632	0.007536	0.704894
-40.111317	-1.911782	1.706637	0.007529	0.704886
-39.748010	-1.973944	1.711642	0.007461	0.704891
-39.831966	-1.958981	1.716646	0.007477	0.704891
-40.282569	-1.984562	1.721651	0.007561	0.704678
-40.481874	-1.989777	1.726656	0.007598	0.704596
-40.974294	-1.906808	1.731661	0.007689	0.704587
-41.012426	-1.896217	1.736666	0.007696	0.704595
-40.937133	-1.911963	1.741670	0.007682	0.704590
-40.825025	-1.933960	1.746675	0.007661	0.704587
-40.642315	-1.962772	1.751680	0.007627	0.704594
-41.326579	-1.990860	1.756685	0.007754	0.704292
-41.773388	-1.923487	1.761690	0.007837	0.704268
-41.623785	-1.952632	1.766694	0.007809	0.704263
-41.847825	-1.915717	1.771699	0.007851	0.704257
-41.892342	-1.903758	1.776704	0.007859	0.704265
-42.199403	-1.853089	1.781709	0.007916	0.704257
-42.069934	-1.871872	1.786714	0.007892	0.704266
-42.002261	-1.955800	1.791718	0.007879	0.704121
-43.131156	-1.838955	1.796723	0.008089	0.703951
-42.763153	-1.900261	1.801728	0.008020	0.703960
-42.882260	-1.884447	1.806733	0.008043	0.703950
-42.749831	-1.904882	1.811738	0.008018	0.703956
-42.602527	-1.931334	1.816742	0.007990	0.703956
-42.925098	-1.877704	1.821747	0.008050	0.703949
-42.483384	-1.977680	1.826752	0.007968	0.703906
-43.122587	-1.999373	1.831757	0.008087	0.703632
-43.616747	-1.909469	1.836762	0.008179	0.703636
-43.809905	-1.875464	1.841766	0.008214	0.703636
-43.530431	-1.927758	1.846771	0.008162	0.703631
-43.656078	-1.901573	1.851776	0.008186	0.703639
-44.073385	-1.832019	1.856781	0.008263	0.703629
-43.462537	-1.945626	1.861786	0.008149	0.703620
-43.817127	-2.020893	1.866790	0.008215	0.703341
-44.548644	-1.895131	1.871795	0.008351	0.703332
-44.373997	-1.922052	1.876800	0.008319	0.703340
-44.243064	-1.948332	1.881805	0.008294	0.703335
-44.658030	-1.872196	1.886810	0.008371	0.703339
-44.180563	-1.956152	1.891814	0.008282	0.703342
-44.114701	-2.040163	1.896819	0.008270	0.703196
-45.558908	-1.874282	1.901824	0.008539	0.703011
-45.367874	-1.913013	1.906829	0.008503	0.703002
-45.239797	-1.934648	1.911834	0.008479	0.703005
-45.170881	-1.946085	1.916838	0.008466	0.703007
-45.573260	-1.876326	1.921843	0.008541	0.703003
-45.066923	-1.962843	1.926848	0.008446	0.703011
-45.085369	-2.040673	1.931853	0.008450	0.702847
-46.474580	-1.871685	1.936858	0.008708	0.702688
-45.945776	-1.963407	1.941862	0.008610	0.702694
-46.036251	-1.951489	1.946867	0.008626	0.702686
-46.256913	-1.907442	1.951872	0.008667	0.702695
-46.138645	-1.932543	1.956877	0.008645	0.702687
-45.834486	-1.983832	1.961882	0.008589	0.702694
-46.231295	-2.031616	1.966886	0.008662	0.702454
-47.224641	-1.899727	1.971891	0.008847	0.702363
-46.926765	-1.946734	1.976896	0.008791	0.702376
-46.909368	-1.955279	1.981901	0.008788	0.702365
-47.315550	-1.880438	1.986906	0.008864	0.702370
-46.971167	-1.942991	1.991910	0.008799	0.702368
-46.922982	-1.954169	1.996915	0.008790	0.702363
-47.787721	-1.925683	2.001920	0.008951	0.702109

-47.772449	-1.946679	2.011917	0.008948	0.702072
-48.101943	-1.887013	2.021914	0.009009	0.702075
-47.824754	-1.937514	2.031910	0.008957	0.702073
-48.038537	-1.899133	2.041907	0.008997	0.702074
-47.948043	-1.916042	2.051904	0.008980	0.702073
-47.869033	-1.928971	2.061901	0.008965	0.702076
-48.030926	-1.900846	2.071898	0.008995	0.702075
-47.850210	-1.934688	2.081894	0.008961	0.702072
-47.992901	-1.910488	2.091891	0.008987	0.702070
-48.003766	-1.906198	2.101888	0.008989	0.702075
-47.876119	-1.928416	2.111885	0.008965	0.702077
-47.286807	-1.901040	2.121882	0.008855	0.702345
-47.103402	-1.923691	2.131878	0.008821	0.702366
-47.196771	-1.906817	2.141875	0.008838	0.702367
-47.002723	-1.940756	2.151872	0.008801	0.702369
-47.086232	-1.924634	2.161869	0.008817	0.702372
-46.885729	-1.904961	2.171866	0.008779	0.702484
-46.180141	-1.929818	2.181862	0.008647	0.702689
-46.269732	-1.914197	2.191859	0.008664	0.702688
-46.267457	-1.912982	2.201856	0.008663	0.702692
-46.207657	-1.916878	2.211853	0.008652	0.702706
-45.615802	-1.874007	2.221850	0.008541	0.703007
-45.365939	-1.922148	2.231846	0.008495	0.703000
-45.463313	-1.904831	2.241843	0.008512	0.703000
-45.211227	-1.929348	2.251840	0.008465	0.703042
-44.676212	-1.876498	2.261837	0.008365	0.703342
-44.426001	-1.922845	2.271834	0.008319	0.703339
-44.444717	-1.920981	2.281830	0.008322	0.703336
-44.628756	-1.829039	2.291827	0.008356	0.703456
-43.680802	-1.910458	2.301824	0.008179	0.703633
-43.524791	-1.938580	2.311821	0.008150	0.703633
-43.748056	-1.898241	2.321818	0.008191	0.703635
-42.970654	-1.901130	2.331814	0.008046	0.703909
-42.889451	-1.897170	2.341811	0.008031	0.703947
-42.723747	-1.925276	2.351808	0.008000	0.703950
-42.860896	-1.854346	2.361805	0.008025	0.704044
-41.834508	-1.932960	2.371802	0.007834	0.704255
-41.820107	-1.935606	2.381798	0.007831	0.704256
-41.898389	-1.922313	2.391795	0.007845	0.704255
-41.344607	-1.914052	2.401792	0.007742	0.704471
-40.980924	-1.920029	2.411789	0.007674	0.704590
-41.139273	-1.892542	2.421786	0.007703	0.704589
-41.035753	-1.890369	2.431782	0.007683	0.704631
-40.356969	-1.885942	2.441779	0.007557	0.704884
-40.131613	-1.925374	2.451776	0.007515	0.704886
-40.289888	-1.896001	2.461773	0.007544	0.704889
-39.594821	-1.903505	2.471770	0.007414	0.705124
-39.255370	-1.922411	2.481766	0.007351	0.705208
-39.266409	-1.920756	2.491763	0.007353	0.705208
-38.903112	-1.985821	2.501760	0.007285	0.705208
-38.573635	-1.889631	2.511757	0.007223	0.705520
-38.292845	-1.937427	2.521754	0.007171	0.705525
-38.385917	-1.922005	2.531750	0.007188	0.705523
-38.177439	-1.894669	2.541747	0.007149	0.705654
-37.136058	-1.977470	2.551744	0.006954	0.705861
-37.293081	-1.947737	2.561741	0.006983	0.705865
-37.346298	-1.939535	2.571738	0.006993	0.705863
-37.054911	-1.898229	2.581734	0.006939	0.706051
-36.866452	-1.894010	2.591731	0.006903	0.706127
-36.494744	-1.959404	2.601728	0.006834	0.706130
-36.654535	-1.865596	2.611725	0.006863	0.706261
-35.449756	-1.990559	2.621722	0.006639	0.706442
-36.003114	-1.892212	2.631718	0.006741	0.706442
-35.571880	-1.970274	2.641715	0.006661	0.706440
-35.105023	-1.913565	2.651712	0.006574	0.706722
-34.977451	-1.919965	2.661709	0.006550	0.706755
-34.915546	-1.931154	2.671706	0.006538	0.706755
-34.705649	-1.880412	2.681702	0.006499	0.706933
-34.241979	-1.887481	2.691699	0.006412	0.707085
-34.113300	-1.912010	2.701696	0.006388	0.707082
-34.158700	-1.870140	2.711693	0.006396	0.707151
-33.124409	-1.942436	2.721690	0.006203	0.707376
-33.443959	-1.885178	2.731686	0.006262	0.707377
-33.383388	-1.895895	2.741683	0.006251	0.707378
-32.658762	-1.876121	2.751680	0.006116	0.707677
-32.405490	-1.908559	2.761677	0.006068	0.707703
-32.556683	-1.880837	2.771674	0.006096	0.707705
-32.019966	-1.882521	2.781670	0.005996	0.707894
-31.437423	-1.925897	2.791667	0.005887	0.708016
-31.595968	-1.896007	2.801664	0.005917	0.708020
-31.440286	-1.915294	2.811661	0.005887	0.708037
-30.391937	-1.945609	2.821658	0.005692	0.708351
-30.557583	-1.916169	2.831654	0.005723	0.708352
-30.296333	-1.962763	2.841651	0.005674	0.708352
-30.799005	-1.825931	2.851648	0.005767	0.708447
-29.594222	-1.942457	2.861645	0.005543	0.708644
-29.787840	-1.908619	2.871642	0.005578	0.708643
-29.608307	-1.941859	2.881638	0.005545	0.708641
-28.762087	-1.960162	2.891635	0.005387	0.708907
-28.805390	-1.927003	2.901632	0.005395	0.708959
-28.795189	-1.928938	2.911629	0.005393	0.708959
-28.857818	-1.879143	2.921626	0.005404	0.709037
-28.271537	-1.870061	2.931622	0.005294	0.709265
-27.913427	-1.934340	2.941619	0.005228	0.709264
-28.133148	-1.894954	2.951616	0.005268	0.709265
-27.086420	-1.917531	2.961613	0.005073	0.709594
-26.921076	-1.944024	2.971610	0.005042	0.709600
-26.852734	-1.956553	2.981606	0.005029	0.709600
-27.113604	-1.876672	2.991603	0.005077	0.709667
-26.116270	-1.940642	3.001600	0.004891	0.709895
-26.045240	-1.951813	3.011597	0.004878	0.709898
-26.314021	-1.903179	3.021594	0.004928	0.709900
-25.623230	-1.901425	3.031590	0.004799	0.710150
-25.230712	-1.937194	3.041587	0.004726	0.710219
-25.316075	-1.921788	3.051584	0.004741	0.710220
-24.989515	-1.949476	3.061581	0.004680	0.710282
-24.574609	-1.897789	3.071578	0.004603	0.710533
-24.054291	-1.990885	3.081574	0.004506	0.710533
-24.500522	-1.911927	3.091571	0.004588	0.710532
-23.987113	-1.897502	3.101568	0.004493	0.710744
-23.336629	-1.949653	3.111565	0.004371	0.710872
-23.436980	-1.931500	3.121562	0.004390	0.710873
-23.272105	-1.962400	3.131558	0.004359	0.710870
-22.619190	-1.951322	3.141555	0.004237	0.711125
-22.675519	-1.935334	3.151552	0.004247	0.711137
-22.619051	-1.945668	3.161549	0.004236	0.711137
-22.594852	-1.866190	3.171546	0.004232	0.711305
-21.641323	-1.960603	3.181542	0.004054	0.711456
-21.989104	-1.899855	3.191539	0.004118	0.711454
-21.771892	-1.913681	3.201536	0.004078	0.711504
-21.049536	-1.912655	3.211533	0.003943	0.711764
-21.000218	-1.922538	3.221530	0.003933	0.711762
-20.948665	-1.932035	3.231526	0.003924	0.711762
-20.548537	-1.865907	3.241523	0.003849	0.712036
-20.032177	-1.930612	3.251520	0.003753	0.712091
-19.854727	-1.961322	3.261517	0.003719	0.712093
-20.047763	-1.880510	3.271514	0.003755	0.712186
-19.254847	-1.920630	3.281510	0.003607	0.712388
-19.273586	-1.917761	3.291507	0.003610	0.712388
-19.255905	-1.920125	3.301504	0.003607	0.712390
-18.426838	-1.909798	3.311501	0.003452	0.712705
-18.338720	-1.922905	3.321498	0.003435	0.712711
-18.080279	-1.968786	3.331494	0.003387	0.712711
-18.408285	-1.845601	3.341491	0.003448	0.712841
-17.204254	-1.968432	3.351488	0.003224	0.713024
-17.613587	-1.893470	3.361485	0.003299	0.713028
-17.637014	-1.886390	3.371482	0.003304	0.713035
-16.832663	-1.864238	3.381478	0.003154	0.713364
-16.647762	-1.898549	3.391475	0.003119	0.713362
-16.631850	-1.900439	3.401472	0.003116	0.713364
-16.397481	-1.843311	3.411469	0.003072	0.713562
-15.958994	-1.874897	3.421466	0.002990	0.713655
-15.819169	-1.901374	3.431462	0.002964	0.713652
-15.844237	-1.838708	3.441459	0.002968	0.713768
-14.737672	-1.933541	3.451456	0.002762	0.713972
-15.001087	-1.886461	3.461453	0.002811	0.713973
-14.902522	-1.902758	3.471450	0.002792	0.713976
-14.309039	-1.870337	3.481446	0.002681	0.714251
-13.931514	-1.923266	3.491443	0.002611	0.714280
-13.852444	-1.937073	3.501440	0.002596	0.714281
-13.923065	-1.883507	3.511437	0.002609	0.714363
-13.072475	-1.910691	3.521434	0.002450	0.714610
-13.046979	-1.916096	3.531430	0.002445	0.714609
-13.141769	-1.899367	3.541427	0.002462	0.714609
-12.564533	-1.892340	3.551424	0.002355	0.714827
-12.488312	-1.863794	3.561421	0.002340	0.714912
-12.201659	-1.916070	3.571418	0.002287	0.714910
-12.192728	-1.866832	3.581414	0.002285	0.715011
-11.241786	-1.924920	3.591411	0.002107	0.715232
-11.231147	-1.926852	3.601408	0.002105	0.715233
-11.375589	-1.898838	3.611405	0.002132	0.715238
-10.813784	-1.891832	3.621402	0.002027	0.715451
-10.452898	-1.906501	3.631398	0.001960	0.715549
-10.569543	-1.887181	3.641395	0.001981	0.715547
-10.269136	-1.926222	3.651392	0.001925	0.715576
-9.879036	-1.839106	3.661389	0.001852	0.715887
-9.334459	-1.935661	3.671386	0.001750	0.715888
-9.801540	-1.853652	3.681382	0.001837	0.715887
-8.985068	-1.923365	3.691379	0.001685	0.716037
-8.367256	-1.985127	3.701376	0.001570	0.716133
-8.485410	-1.961793	3.711373	0.001591	0.716138
-8.518911	-1.957796	3.721370	0.001597	0.716135
-7.898014	-1.947239	3.731366	0.001481	0.716375
-7.513126	-1.979684	3.741363	0.001410	0.716447
-7.307860	-2.016199	3.751360	0.001371	0.716448
-7.383080	-2.001892	3.761357	0.001385	0.716450
-6.650351	-2.008430	3.771354	0.001248	0.716696
-6.833212	-1.944519	3.781350	0.001282	0.716758
-6.568202	-1.991476	3.791347	0.001232	0.716759
-6.366840	-2.028440	3.801344	0.001195	0.716758
-5.812503	-1.969108	3.811341	0.001091	0.717071
-5.574032	-2.005334	3.821338	0.001047	0.717084
-5.865502	-1.952871	3.831334	0.001100	0.717085
-5.580007	-1.963623	3.841331	0.001047	0.717165
-4.718790	-2.007012	3.851328	0.000887	0.717383
-4.716860	-2.007155	3.861325	0.000886	0.717384
-4.667400	-2.017699	3.871322	0.000876	0.717381
-4.438466	-1.960466	3.881318	0.000834	0.717575
-3.782116	-2.012960	3.891315	0.000711	0.717703
-3.779885	-2.011654	3.901312	0.000710	0.717707
-3.731021	-2.019444	3.911309	0.000701	0.717709
-3.265122	-1.962525	3.921306	0.000614	0.717986
-3.026055	-1.986468	3.931302	0.000569	0.718024
-2.752900	-2.035740	3.941299	0.000518	0.718023
-3.086933	-1.922623	3.951296	0.000580	0.718129
-2.323202	-1.940534	3.961293	0.000438	0.718363
-2.291261	-1.947682	3.971290	0.000432	0.718360
-2.401853	-1.912317	3.981286	0.000452	0.718392
-1.620439	-1.921770	3.991283	0.000306	0.718648
-1.564572	-1.931794	4.001280	0.000295	0.718649
-1.603758	-1.925525	4.011277	0.000303	0.718648
-1.320218	-1.823227	4.021274	0.000249	0.718950
-1.524847	-1.778431	4.031270	0.000287	0.718967
-1.260110	-1.783588	4.041267	0.000238	0.719050
-1.333215	-1.652206	4.051264	0.000251	0.719284
-1.289513	-1.651149	4.061261	0.000243	0.719302
-1.042562	-1.538308	4.071258	0.000196	0.719612
-0.908883	-1.563891	4.081254	0.000171	0.719609
-1.009052	-1.404362	4.091251	0.000190	0.719888
-0.879184	-1.405196	4.101248	0.000165	0.719933
-0.828598	-1.262171	4.111245	0.000155	0.720233
-0.527413	-1.263423	4.121242	0.000099	0.720337
-0.623269	-1.138414	4.131238	0.000117	0.720550
-0.869825	-0.980588	4.141235	0.000162	0.720774
-0.942634	-0.878004	4.151232	0.000175	0.720951
-0.671984	-0.833370	4.161229	0.000125	0.721134
-0.470780	-0.734151	4.171226	0.000087	0.721400
-0.200843	-0.684202	4.181222	0.000036	0.721594
-0.253641	-0.578399	4.191219	0.000046	0.721784
-0.004537	-0.470400	4.201216	-0.000001	0.722083
-0.134508	-0.328075	4.211213	0.000023	0.722318
-0.209030	-0.185434	4.221210	0.000037	0.722573
-0.368465	-0.020267	4.231206	0.000066	0.722842
-0.099410	0.075883	4.241203	0.000015	0.723125
0.000000	0.233610	4.251200	-0.000003	0.723469

0.350029	0.789433	4.256205	-0.000069	0.724681
0.581846	2.020502	4.261210	-0.000113	0.727168
0.863317	3.836956	4.266214	-0.000167	0.730800
1.152040	6.205793	4.271219	-0.000222	0.735484
1.726345	9.040366	4.276224	-0.000331	0.741128
2.085997	12.393554	4.281229	-0.000400	0.747640
2.692944	16.156450	4.286234	-0.000516	0.754950
3.124614	20.359461	4.291238	-0.000599	0.762950
3.608704	24.951679	4.296243	-0.000693	0.771600
4.211142	29.895399	4.301248	-0.000808	0.780831
4.903558	35.166901	4.306253	-0.000941	0.790570
5.556988	40.773022	4.311258	-0.001066	0.800772
6.101993	46.699177	4.316262	-0.001171	0.811371
6.669527	52.899114	4.321267	-0.001281	0.822313
9.280873	59.040540	4.326272	-0.001772	0.833625
10.066624	65.733920	4.331277	-0.001922	0.845170
10.527285	72.716828	4.336282	-0.002013	0.856943
11.283684	79.845541	4.341286	-0.002158	0.868880
11.686638	87.220128	4.346291	-0.002238	0.880951
12.492840	94.705194	4.351296	-0.002394	0.893146
13.188205	102.357473	4.356301	-0.002528	0.905407
13.804615	110.178658	4.361306	-0.002648	0.917745
14.394036	118.102461	4.366310	-0.002763	0.930067
16.488440	125.881206	4.371315	-0.003158	0.942406
17.171425	134.040976	4.376320	-0.003291	0.954783
17.782206	142.274666	4.381325	-0.003410	0.967092
18.521397	150.585580	4.386330	-0.003553	0.979390
19.456631	158.946847	4.391334	-0.003733	0.991656
20.332627	167.362584	4.396339	-0.003902	1.003834
20.937985	175.865911	4.401344	-0.004020	1.015922
21.783854	184.346699	4.406349	-0.004183	1.027894
22.617242	192.890285	4.411354	-0.004344	1.039810
23.312090	201.473311	4.416358	-0.004479	1.051611
24.075414	210.074084	4.421363	-0.004627	1.063321
25.134047	218.670452	4.426368	-0.004830	1.074964
25.610738	227.335097	4.431373	-0.004925	1.086440
26.413195	235.976197	4.436378	-0.005080	1.097837
27.363659	244.591198	4.441382	-0.005262	1.109117
28.027791	253.256221	4.446387	-0.005392	1.120283
28.583270	261.932639	4.451392	-0.005501	1.131330
29.315208	270.566290	4.456397	-0.005643	1.142253
29.993757	279.251292	4.461402	-0.005775	1.153125
30.518476	287.904516	4.466406	-0.005879	1.163825
31.166872	296.527543	4.471411	-0.006005	1.174415
31.862766	305.130544	4.476416	-0.006140	1.184896
32.458621	313.747102	4.481421	-0.006257	1.195281
33.562439	322.265275	4.486426	-0.006468	1.205562
34.301863	330.841856	4.491430	-0.006612	1.215752
34.838440	339.427731	4.496435	-0.006717	1.225827
35.287676	348.055275	4.501440	-0.006807	1.235851
35.793048	356.590407	4.506445	-0.006907	1.245699
36.637306	365.100282	4.511450	-0.007069	1.255506
37.184845	373.625069	4.516454	-0.007177	1.265198
37.719315	382.150259	4.521459	-0.007282	1.274813
38.423909	390.628392	4.526464	-0.007419	1.284336
39.037782	399.109335	4.531469	-0.007539	1.293775
39.680450	407.590081	4.536474	-0.007664	1.303150
40.133531	416.169910	4.541478	-0.007754	1.312530
40.610777	424.642886	4.546483	-0.007849	1.321734
41.415998	433.014615	4.551488	-0.008004	1.330824
41.521519	441.491454	4.556493	-0.008030	1.339840
42.000849	449.895047	4.561498	-0.008125	1.348784
42.384021	458.317263	4.566502	-0.008202	1.357671
42.781624	466.691235	4.571507	-0.008281	1.366453
43.389889	475.065836	4.576512	-0.008400	1.375216
43.875119	483.413638	4.581517	-0.008496	1.383874
44.516951	491.783359	4.586522	-0.008621	1.392527
45.591848	500.035978	4.591526	-0.008827	1.401081
46.117207	508.388443	4.596531	-0.008930	1.409591
46.475201	516.770071	4.601536	-0.009002	1.418051
47.302285	525.036787	4.606541	-0.009162	1.426424
48.085822	533.348176	4.611546	-0.009313	1.434785
48.688865	541.655801	4.616550	-0.009431	1.443064
48.933913	550.020244	4.621555	-0.009482	1.451293
49.483164	558.339058	4.626560	-0.009590	1.459480
49.998089	566.639256	4.631565	-0.009691	1.467598
50.733107	574.967362	4.636570	-0.009834	1.475732
51.205569	583.236519	4.641574	-0.009927	1.483725
52.123454	591.464693	4.646579	-0.010104	1.491704
52.489172	599.780896	4.651584	-0.010177	1.499639
53.121630	608.023968	4.656589	-0.010301	1.507503
53.884782	616.278836	4.661594	-0.010448	1.515358
54.233327	624.562423	4.666598	-0.010519	1.523136
54.694779	632.829707	4.671603	-0.010610	1.530876
55.150190	641.109602	4.676608	-0.010700	1.538588
55.583072	649.348090	4.681613	-0.010787	1.546219
56.051931	657.638663	4.686618	-0.010879	1.553866
56.327437	665.889093	4.691622	-0.010936	1.561411
57.158722	674.060562	4.696627	-0.011096	1.568928
57.651468	682.316421	4.701632	-0.011194	1.576437
57.987985	690.558027	4.706637	-0.011262	1.583874
58.471240	698.794367	4.711642	-0.011357	1.591293
59.003419	707.008709	4.716646	-0.011462	1.598665
59.331609	715.231352	4.721651	-0.011528	1.605981
60.136399	723.408826	4.726656	-0.011684	1.613291
60.610286	731.610330	4.731661	-0.011777	1.620543
61.001154	739.848434	4.736666	-0.011856	1.627782
61.443813	748.122649	4.741670	-0.011944	1.635028
61.637753	756.333141	4.746675	-0.011985	1.642152
62.236785	764.503988	4.751680	-0.012102	1.649267
62.698920	772.690970	4.756685	-0.012194	1.656346
63.438794	780.837719	4.761690	-0.012337	1.663399
64.093587	789.012949	4.766694	-0.012464	1.670434
64.437803	797.228212	4.771699	-0.012534	1.677431
65.014936	805.409611	4.776704	-0.012647	1.684402
65.683444	813.566203	4.781709	-0.012777	1.691335
66.110795	821.764365	4.786714	-0.012862	1.698243
66.281182	829.976751	4.791718	-0.012899	1.705100
66.631468	838.190714	4.796723	-0.012970	1.711955
67.164868	846.353533	4.801728	-0.013074	1.718764
67.494602	854.503683	4.806733	-0.013141	1.725509
67.911655	862.685589	4.811738	-0.013224	1.732265
68.294904	870.856509	4.816742	-0.013301	1.738982
68.554834	879.021197	4.821747	-0.013355	1.745651
69.200612	887.172801	4.826752	-0.013481	1.752334
69.703832	895.309612	4.831757	-0.013580	1.758961
70.198595	903.458139	4.836762	-0.013677	1.765571
70.500158	911.651376	4.841766	-0.013739	1.772168
70.921843	919.802897	4.846771	-0.013823	1.778722
71.635434	927.919567	4.851776	-0.013961	1.785260
71.971410	936.131362	4.856781	-0.014029	1.791804
72.846168	944.238215	4.861786	-0.014197	1.798306
73.393067	952.348768	4.866790	-0.014305	1.804747
73.839169	960.498423	4.871795	-0.014393	1.811184
74.394646	968.645040	4.876800	-0.014502	1.817609
74.942438	976.762503	4.881805	-0.014609	1.823988
75.412869	984.924054	4.886810	-0.014703	1.830368
75.752717	993.090469	4.891814	-0.014771	1.836715
76.266716	1001.208993	4.896819	-0.014872	1.843024
76.922123	1009.343562	4.901824	-0.015000	1.849340
77.294008	1017.505551	4.906829	-0.015075	1.855622
77.747955	1025.649783	4.911834	-0.015164	1.861878
78.154903	1033.799573	4.916838	-0.015246	1.868113
78.654771	1041.947126	4.921843	-0.015344	1.874335
79.072099	1050.074669	4.926848	-0.015427	1.880512
79.675156	1058.154938	4.931853	-0.015545	1.886655
80.127830	1066.307262	4.936858	-0.015635	1.892814
80.630639	1074.415535	4.941862	-0.015734	1.898926
80.882530	1082.558348	4.946867	-0.015786	1.905016
81.389869	1090.706554	4.951872	-0.015886	1.911118
81.614655	1098.844663	4.956877	-0.015933	1.917163
82.062458	1106.955334	4.961882	-0.016022	1.923192
82.454801	1115.084485	4.966886	-0.016101	1.929210
82.729046	1123.234739	4.971891	-0.016157	1.935212
83.324756	1131.327395	4.976896	-0.016273	1.941188
83.770529	1139.428724	4.981901	-0.016362	1.947136
84.379084	1147.573495	4.986906	-0.016480	1.953115
84.747607	1155.700389	4.991910	-0.016555	1.959036
85.048555	1163.789066	4.996915	-0.016616	1.964905
85.746405	1171.865165	5.001920	-0.016751	1.970789
86.006239	1179.995301	5.006925	-0.016805	1.976648
86.418741	1188.107631	5.011930	-0.016887	1.982493
87.091684	1196.183429	5.016934	-0.017018	1.988322
87.439547	1204.320530	5.021939	-0.017088	1.994143
87.915687	1212.411543	5.026944	-0.017182	1.999928
88.317165	1220.501615	5.031949	-0.017262	2.005688
88.712185	1228.644199	5.036954	-0.017341	2.011467
88.995992	1236.783358	5.041958	-0.017400	2.017216
89.241903	1244.892676	5.046963	-0.017451	2.022923
89.837205	1252.982421	5.051968	-0.017567	2.028637
89.984219	1261.152842	5.056973	-0.017600	2.034344
90.362329	1269.231432	5.061978	-0.017676	2.039996
90.618474	1277.319267	5.066982	-0.017729	2.045626
90.891849	1285.424144	5.071987	-0.017785	2.051253
91.209033	1293.546475	5.076992	-0.017850	2.056882
91.509637	1301.615270	5.081997	-0.017911	2.062457
92.055082	1309.688476	5.087002	-0.018018	2.068044
92.406313	1317.819563	5.092006	-0.018089	2.073636
92.544699	1325.908213	5.097011	-0.018120	2.079163
92.961718	1333.993003	5.102016	-0.018203	2.084700
93.299030	1342.081450	5.107021	-0.018271	2.090217
93.731814	1350.188590	5.112026	-0.018357	2.095742
94.168116	1358.260186	5.117030	-0.018444	2.101228
94.533078	1366.341693	5.122035	-0.018517	2.106699
94.900386	1374.508707	5.127040	-0.018591	2.112214
95.061898	1382.625860	5.132045	-0.018626	2.117661
95.468172	1390.679911	5.137050	-0.018707	2.123076
95.976271	1398.728722	5.142054	-0.018807	2.128482
96.294128	1406.832749	5.147059	-0.018872	2.133894
96.801387	1414.906648	5.152064	-0.018972	2.139290
97.132984	1422.975355	5.157069	-0.019039	2.144652
97.627098	1431.060049	5.162074	-0.019136	2.150026
98.156352	1439.146560	5.167078	-0.019240	2.155391
98.570180	1447.198090	5.172083	-0.019323	2.160710
99.099430	1455.283713	5.177088	-0.019427	2.166048
99.282212	1463.392431	5.182093	-0.019466	2.171355
99.630280	1471.500822	5.187098	-0.019536	2.176665
99.903024	1479.583870	5.192102	-0.019592	2.181938
100.293585	1487.655067	5.197107	-0.019671	2.187202
100.695757	1495.788393	5.202112	-0.019751	2.192494
100.954748	1503.871439	5.207117	-0.019804	2.197728
101.493577	1511.914862	5.212122	-0.019910	2.202949
101.924180	1519.992023	5.217126	-0.019996	2.208170
102.172772	1528.087817	5.222131	-0.020047	2.213374
102.341375	1536.205265	5.227136	-0.020084	2.218572
102.442897	1544.268849	5.232141	-0.020109	2.223718
103.078443	1552.327421	5.237146	-0.020232	2.228896
103.469848	1560.425003	5.242150	-0.020310	2.234064
103.728297	1568.496190	5.247155	-0.020364	2.239193
104.282763	1576.544613	5.252160	-0.020473	2.244321
104.471588	1584.627456	5.257165	-0.020513	2.249428
104.716317	1592.748911	5.262170	-0.020564	2.254551
105.031826	1600.801429	5.267174	-0.020628	2.259626
105.458888	1608.850095	5.272179	-0.020713	2.264697
105.704340	1616.978289	5.277184	-0.020764	2.269790
106.146555	1625.106047	5.282189	-0.020852	2.274889
106.609080	1633.127555	5.287194	-0.020944	2.279911
106.939526	1641.180732	5.292198	-0.021010	2.284931
107.043331	1649.250678	5.297203	-0.021035	2.289931
107.623719	1657.316228	5.302208	-0.021149	2.294958
107.853137	1665.376927	5.307213	-0.021197	2.299940
108.277640	1673.428832	5.312218	-0.021281	2.304923
108.692091	1681.508253	5.317222	-0.021364	2.309912
109.255323	1689.563166	5.322227	-0.021474	2.314886
109.606852	1697.642644	5.327232	-0.021545	2.319848
109.722058	1705.722576	5.332237	-0.021572	2.324779
109.975392	1713.799187	5.337242	-0.021624	2.329709
110.360501	1721.891702	5.342246	-0.021701	2.334650
110.560862	1729.949728	5.347251	-0.021744	2.339543
110.844030	1738.031941	5.352256	-0.021802	2.344448
111.238669	1746.070077	5.357261	-0.021881	2.349325
111.409165	1754.217784	5.362266	-0.021918	2.354240
111.728615	1762.252195	5.367270	-0.021983	2.359088
112.256206	1770.257887	5.372275	-0.022086	2.363926
112.491225	1778.357804	5.377280	-0.022136	2.368787
112.657980	1786.447535	5.382285	-0.022172	2.373626
113.077997	1794.506860	5.387290	-0.022256	2.378457
113.237701	1802.575324	5.392294	-0.022291	2.383263
113.251934	1810.660114	5.397299	-0.022299	2.388058
113.804442	1818.717669	5.402304	-0.022407	2.392869
114.162622	1826.771910	5.407309	-0.022479	2.397653
114.360645	1834.835405	5.412314	-0.022521	2.402421
114.583109	1842.888438	5.417318	-0.022568	2.407175
114.959533	1850.954712	5.422323	-0.022644	2.411939
115.434316	1859.033247	5.427328	-0.022737	2.416708
115.526499	1867.096573	5.432333	-0.022760	2.421430
115.951132	1875.139076	5.437338	-0.022844	2.426156
116.450042	1883.218082	5.442342	-0.022943	2.430899
116.446588	1891.359930	5.447347	-0.022947	2.435631
116.672839	1899.405033	5.452352	-0.022995	2.440316
116.833362	1907.407986	5.457357	-0.023030	2.444962
117.198395	1915.446539	5.462362	-0.023104	2.449635
117.639321	1923.520023	5.467366	-0.023191	2.454325
117.845052	1931.566942	5.472371	-0.023235	2.458973
118.359898	1939.602530	5.477376	-0.023336	2.463629
118.375253	1947.681076	5.482381	-0.023344	2.468263
118.731205	1955.746938	5.487386	-0.023416	2.472907
119.230633	1963.782509	5.492390	-0.023514	2.477535
119.685589	1971.803305	5.497395	-0.023604	2.482143
119.857342	1979.894883	5.502400	-0.023642	2.486761
120.372457	1987.932245	5.507405	-0.023743	2.491366
120.764617	1996.004805	5.512410	-0.023821	2.495972
120.743602	2004.096612	5.517414	-0.023823	2.500551
121.041613	2012.133469	5.522419	-0.023884	2.505114
121.650333	2020.204850	5.527424	-0.024002	2.509710
121.750829	2028.295785	5.532429	-0.024026	2.514272
121.909189	2036.359048	5.537434	-0.024061	2.518815
122.342121	2044.384898	5.542438	-0.024147	2.523347
122.605774	2052.413851	5.547443	-0.024202	2.527862
122.918311	2060.484648	5.552448	-0.024265	2.532395
123.126867	2068.562894	5.557453	-0.024310	2.536916
123.486029	2076.591115	5.562458	-0.024382	2.541413
123.776655	2084.634607	5.567462	-0.024441	2.545904
124.035598	2092.695662	5.572467	-0.024495	2.550396
124.396921	2100.768872	5.577472	-0.024567	2.554893
124.501853	2108.812331	5.582477	-0.024592	2.559348
124.706867	2116.877079	5.587482	-0.024636	2.563814
125.256152	2124.908458	5.592486	-0.024744	2.568278
125.146080	2133.002901	5.597491	-0.024728	2.572723
125.419972	2141.066826	5.602496	-0.024785	2.577170
126.063880	2149.066314	5.607501	-0.024910	2.581599
126.298932	2157.126780	5.612506	-0.024959	2.586026
126.467534	2165.224091	5.617510	-0.024996	2.590461
126.605357	2173.470154	5.622515	-0.025027	2.594968
127.241268	2181.422433	5.627520	-0.025151	2.599340
127.490637	2189.404608	5.632525	-0.025203	2.603695
127.557315	2197.456946	5.637530	-0.025220	2.608069
127.888241	2205.487239	5.642534	-0.025287	2.612440
128.443829	2213.495613	5.647539	-0.025396	2.616808
128.805191	2221.531269	5.652544	-0.025469	2.621170
128.902484	2229.582936	5.657549	-0.025492	2.625516
129.301126	2237.622542	5.662554	-0.025572	2.629868
129.611787	2245.705429	5.667558	-0.025635	2.634230
129.792931	2253.737388	5.672563	-0.025674	2.638549
130.292833	2261.764890	5.677568	-0.025773	2.642880
130.408022	2269.823382	5.682573	-0.025799	2.647195
130.666221	2277.876178	5.687578	-0.025853	2.651509
131.086152	2285.941308	5.692582	-0.025936	2.655833
131.385500	2293.962843	5.697587	-0.025998	2.660119
131.593457	2302.025078	5.702592	-0.026042	2.664413
131.649603	2310.092344	5.707597	-0.026058	2.668694
132.253036	2318.128768	5.712602	-0.026175	2.672986
132.490512	2326.211480	5.717606	-0.026225	2.677273
132.366856	2334.260865	5.722611	-0.026207	2.681512
132.699735	2342.291047	5.727616	-0.026275	2.685763
132.993004	2350.312781	5.732621	-0.026334	2.690001
133.231865	2358.396720	5.737626	-0.026384	2.694260
133.504325	2366.428189	5.742630	-0.026440	2.698488
133.819038	2374.427369	5.747635	-0.026504	2.702695
134.108364	2382.497838	5.752640	-0.026564	2.706931
134.235310	2390.554393	5.757645	-0.026593	2.711143
134.577654	2398.630887	5.762650	-0.026662	2.715372
134.874640	2406.649891	5.767654	-0.026722	2.719562
135.047448	2414.675731	5.772659	-0.026760	2.723741
135.610697	2422.699661	5.777664	-0.026870	2.727937
135.926855	2430.738964	5.782669	-0.026934	2.732119
136.309839	2438.817331	5.787674	-0.027011	2.736318
136.572444	2446.865031	5.792678	-0.027065	2.740488
136.872037	2454.876540	5.797683	-0.027126	2.744636
137.153643	2462.974711	5.802688	-0.027184	2.748820
137.532814	2471.079417	5.807693	-0.027260	2.753007
137.966874	2479.108652	5.812698	-0.027347	2.757153
138.427022	2487.109363	5.817702	-0.027438	2.761279
138.768136	2495.114216	5.822707	-0.027506	2.765393
139.201198	2503.159019	5.827712	-0.027592	2.769528
139.629084	2511.222826	5.832717	-0.027677	2.773666
139.697932	2519.298907	5.837722	-0.027696	2.777782
140.158338	2527.315802	5.842726	-0.027787	2.781885
140.285986	2535.351320	5.847731	-0.027816	2.785972
140.547657	2543.430071	5.852736	-0.027870	2.790083
140.942095	2551.446939	5.857741	-0.027949	2.794164
141.139027	2559.496650	5.862746	-0.027991	2.798244
141.408232	2567.518968	5.867750	-0.028046	2.802309
141.668012	2575.554173	5.872755	-0.028100	2.806373
142.086314	2583.590469	5.877760	-0.028183	2.810441
142.310523	2591.654014	5.882765	-0.028230	2.814506
142.511901	2599.709541	5.887770	-0.028273	2.818560
142.814444	2607.742806	5.892774	-0.028335	2.822602
143.037619	2615.783683	5.897779	-0.028382	2.826638
143.498103	2623.830489	5.902784	-0.028473	2.830685
143.512650	2631.941520	5.907789	-0.028481	2.834732
143.696952	2639.939586	5.912794	-0.028521	2.838727
144.105741	2647.954434	5.917798	-0.028602	2.842737
144.178349	2655.992971	5.922803	-0.028621	2.846734
144.494049	2664.043192	5.927808	-0.028685	2.850746
144.870243	2672.085520	5.932813	-0.028761	2.854750
145.132297	2680.103534	5.937818	-0.028815	2.858731
145.413323	2688.150358	5.942822	-0.028872	2.862722
145.700271	2696.174344	5.947827	-0.028931	2.866696
146.150530	2704.234527	5.952832	-0.029020	2.870691
146.281204	2712.311321	5.957837	-0.029050	2.874671
146.404784	2720.326402	5.962842	-0.029079	2.878615
146.866392	2728.351319	5.967846	-0.029170	2.882577
146.853498	2736.394850	5.972851	-0.029173	2.886517
147.395343	2744.410984	5.977856	-0.029279	2.890468
147.699250	2752.477459	5.982861	-0.029341	2.894425
147.989866	2760.497697	5.987866	-0.029400	2.898353
148.135264	2768.562918	5.992870	-0.029433	2.902290
148.160273	2776.615161	5.997875	-0.029443	2.906210
148.690229	2784.641570	6.002880	-0.029547	2.910138
148.713372	2792.804132	6.007885	-0.029557	2.914099
149.147202	2800.764030	6.012890	-0.029643	2.917979
149.633971	2808.767726	6.017894	-0.029739	2.921878
149.534305	2816.808084	6.022899	-0.029726	2.925759
149.840082	2824.822778	6.027904	-0.029788	2.929643
150.249964	2832.866156	6.032909	-0.029870	2.933541
150.634550	2840.879714	6.037914	-0.029947	2.937418
150.907164	2848.938274	6.042918	-0.030003	2.941306
151.149786	2856.939300	6.047923	-0.030053	2.945159
151.389705	2865.020307	6.052928	-0.030103	2.949046
151.851164	2873.065461	6.057933	-0.030195	2.952922
152.105632	2881.106406	6.062938	-0.030247	2.956779
152.377417	2889.132590	6.067942	-0.030303	2.960626
152.528902	2897.165193	6.072947	-0.030337	2.964465
152.518226	2905.222319	6.077952	-0.030340	2.968301
152.746048	2913.256589	6.082957	-0.030388	2.972135
153.208790	2921.290854	6.087962	-0.030479	2.975975
153.532879	2929.294493	6.092966	-0.030545	2.979788
153.717616	2937.329257	6.097971	-0.030585	2.983605
154.004265	2945.386085	6.102976	-0.030644	2.987432
154.218972	2953.439844	6.107981	-0.030689	2.991248
154.517969	2961.494471	6.112986	-0.030750	2.995065
154.680690	2969.535427	6.117990	-0.030786	2.998864
154.876879	2977.516804	6.122995	-0.030828	3.002631
154.931524	2985.586257	6.128000	-0.030843	3.006428
155.129833	2993.594384	6.133005	-0.030885	3.010198
155.648012	3001.635905	6.138010	-0.030987	3.013995
155.799773	3009.690659	6.143014	-0.031021	3.017776
156.017692	3017.717340	6.148019	-0.031067	3.021542
156.451279	3025.724426	6.153024	-0.031153	3.025304
156.758876	3033.776852	6.158029	-0.031216	3.029077
156.825821	3041.850283	6.163034	-0.031233	3.032843
157.171399	3049.908404	6.168038	-0.031303	3.036610
157.328920	3057.874462	6.173043	-0.031338	3.040321
157.640088	3065.917303	6.178048	-0.031401	3.044071
157.757675	3073.953038	6.183053	-0.031428	3.047803
158.041342	3081.993829	6.188058	-0.031486	3.051541
158.345766	3090.062095	6.193062	-0.031549	3.055288
158.521858	3098.048051	6.198067	-0.031587	3.058987
158.849974	3106.102755	6.203072	-0.031653	3.062719
158.836943	3114.128924	6.208077	-0.031656	3.066418
159.146203	3122.166714	6.213082	-0.031719	3.070133
159.537937	3130.286229	6.218086	-0.031797	3.073885
159.791282	3138.292448	6.223091	-0.031850	3.077573
159.991202	3146.326734	6.228096	-0.031892	3.081268
160.175985	3154.325930	6.233101	-0.031932	3.084941
160.514389	3162.326848	6.238106	-0.032001	3.088618
161.053413	3170.363171	6.243110	-0.032106	3.092316
160.888578	3178.429836	6.248115	-0.032081	3.095991
161.331668	3186.424091	6.253120	-0.032169	3.099656
161.542841	3194.465549	6.258125	-0.032213	3.103328
161.791214	3202.515009	6.263130	-0.032265	3.107000
161.975618	3210.562598	6.268134	-0.032305	3.110665
162.173089	3218.593015	6.273139	-0.032347	3.114318
162.567588	3226.622456	6.278144	-0.032426	3.117975
163.144304	3234.623550	6.283149	-0.032538	3.121623
163.527860	3242.609797	6.288154	-0.032615	3.125252
163.768984	3250.683149	6.293158	-0.032665	3.128909
163.765884	3258.765094	6.298163	-0.032670	3.132555
164.167132	3266.808578	6.303168	-0.032750	3.136197
164.485848	3274.798194	6.308173	-0.032815	3.139807
164.739992	3282.800686	6.313178	-0.032868	3.143416
165.427284	3290.822560	6.318182	-0.033001	3.147048
165.691000	3298.867310	6.323187	-0.033055	3.150667
166.084363	3306.944456	6.328192	-0.033134	3.154303
166.075741	3314.991099	6.333197	-0.033138	3.157903
166.567952	3322.977648	6.338202	-0.033235	3.161494
166.773079	3330.999070	6.343206	-0.033278	3.165084
166.823883	3339.020719	6.348211	-0.033293	3.168663
167.139551	3347.110233	6.353216	-0.033357	3.172280
167.529085	3355.124847	6.358221	-0.033435	3.175863
167.566702	3363.160526	6.363226	-0.033448	3.179436
168.018038	3371.163738	6.368230	-0.033537	3.183008
168.132221	3379.199074	6.373235	-0.033564	3.186575
168.363170	3387.252853	6.378240	-0.033612	3.190152
168.773563	3395.307274	6.383245	-0.033694	3.193733
168.916993	3403.350936	6.388250	-0.033726	3.197294
169.308558	3411.354060	6.393254	-0.033804	3.200843
169.248658	3419.369082	6.398259	-0.033798	3.204374
169.560419	3427.414759	6.403264	-0.033862	3.207931
169.779086	3435.463341	6.408269	-0.033908	3.211481
169.839127	3443.499528	6.413274	-0.033924	3.215015
170.172541	3451.526201	6.418278	-0.033992	3.218552
170.497229	3459.519946	6.423283	-0.034058	3.222071
170.797474	3467.528434	6.428288	-0.034119	3.225591
171.197792	3475.590806	6.433293	-0.034199	3.229135
171.531605	3483.641950	6.438298	-0.034266	3.232667
172.037954	3491.706178	6.443302	-0.034366	3.236208
171.855463	3499.693970	6.448307	-0.034337	3.239684
172.077758	3507.720448	6.453312	-0.034384	3.243189
172.451545	3515.728189	6.458317	-0.034459	3.246689
172.640382	3523.732947	6.463322	-0.034499	3.250176
172.721703	3531.823128	6.468326	-0.034520	3.253692
173.142905	3539.816947	6.473331	-0.034604	3.257175
173.168128	3547.864207	6.478336	-0.034614	3.260663
173.357443	3555.882114	6.483341	-0.034654	3.264141
173.649913	3563.892827	6.488346	-0.034714	3.267615
173.935791	3571.964166	6.493350	-0.034773	3.271112
174.032075	3580.008529	6.498355	-0.034796	3.274586
174.393585	3588.020956	6.503360	-0.034869	3.278053
174.646922	3596.025638	6.508365	-0.034921	3.281509
174.644462	3604.044371	6.513370	-0.034926	3.284957
174.822859	3612.109178	6.518374	-0.034965	3.288429
175.219616	3620.129642	6.523379	-0.035044	3.291886
175.400089	3628.169970	6.528384	-0.035083	3.295339
175.875126	3636.175895	6.533389	-0.035177	3.298786
176.231973	3644.184107	6.538394	-0.035249	3.302225
176.523097	3652.235167	6.543398	-0.035308	3.305676
176.587500	3660.256247	6.548403	-0.035325	3.309103
176.977189	3668.312723	6.553408	-0.035403	3.312553
177.405932	3676.348701	6.558413	-0.035489	3.315992
177.401332	3684.357798	6.563418	-0.035493	3.319400
177.687554	3692.387184	6.568422	-0.035552	3.322824
177.894634	3700.381881	6.573427	-0.035596	3.326227
178.109527	3708.415854	6.578432	-0.035641	3.329643
178.348657	3716.478933	6.583437	-0.035691	3.333068
178.669921	3724.507900	6.588442	-0.035756	3.336479
178.953644	3732.510082	6.593446	-0.035814	3.339874
178.940246	3740.558740	6.598451	-0.035817	3.343274
179.224433	3748.578146	6.603456	-0.035875	3.346669
179.599634	3756.600990	6.608461	-0.035951	3.350065
179.718274	3764.661552	6.613466	-0.035978	3.353464
179.831064	3772.731600	6.618470	-0.036004	3.356863
180.026666	3780.682442	6.623475	-0.036046	3.360212
180.582581	3788.709605	6.628480	-0.036155	3.363603
180.723317	3796.759524	6.633485	-0.036187	3.366985
180.677645	3804.781215	6.638490	-0.036183	3.370345
181.175425	3812.857515	6.643494	-0.036281	3.373743
181.238599	3820.892935	6.648499	-0.036299	3.377106
181.595124	3828.873609	6.653504	-0.036370	3.380453
181.877688	3836.877553	6.658509	-0.036428	3.383803
182.037082	3844.892387	6.663514	-0.036463	3.387151
182.139591	3852.950727	6.668518	-0.036488	3.390511
182.290236	3861.032625	6.673523	-0.036521	3.393879
182.687357	3869.076605	6.678528	-0.036601	3.397237
182.818027	3877.056811	6.683533	-0.036630	3.400556
182.757808	3885.047116	6.688538	-0.036624	3.403869
183.119273	3893.106102	6.693542	-0.036697	3.407221
183.137019	3901.092869	6.698547	-0.036706	3.410529
183.521809	3909.126735	6.703552	-0.036783	3.413866
183.511785	3917.195699	6.708557	-0.036786	3.417200
183.764846	3925.174637	6.713562	-0.036839	3.420503
184.047736	3933.216536	6.718566	-0.036897	3.423829
184.135758	3941.237520	6.723571	-0.036918	3.427137
184.609118	3949.235800	6.728576	-0.037012	3.430446
184.704673	3957.338685	6.733581	-0.037035	3.433781
184.923174	3965.330100	6.738586	-0.037081	3.437072
185.118037	3973.360865	6.743590	-0.037123	3.440375
185.306885	3981.358797	6.748595	-0.037163	3.443660
185.407828	3989.404294	6.753600	-0.037187	3.446960
185.833229	3997.403377	6.758605	-0.037272	3.450248
186.077757	4005.469793	6.763610	-0.037323	3.453554
186.222795	4013.551977	6.768614	-0.037355	3.456860
186.354429	4021.511391	6.773619	-0.037385	3.460112
186.533602	4029.548912	6.778624	-0.037424	3.463395
186.711885	4037.601121	6.783629	-0.037462	3.466681
186.784792	4045.617935	6.788634	-0.037481	3.469946
187.169973	4053.682340	6.793638	-0.037558	3.473236
187.435411	4061.691678	6.798643	-0.037613	3.476498
187.597156	4069.689835	6.803648	-0.037649	3.479749
187.577963	4077.725071	6.808653	-0.037650	3.483005
187.843051	4085.703299	6.813658	-0.037705	3.486245
188.218415	4093.720661	6.818662	-0.037780	3.489501
188.354345	4101.744135	6.823667	-0.037811	3.492749
188.736909	4109.804058	6.828672	-0.037887	3.496016
188.879806	4117.808881	6.833677	-0.037919	3.499251
189.133175	4125.815798	6.838682	-0.037972	3.502486
189.367015	4133.863537	6.843686	-0.038021	3.505735
189.688912	4141.846145	6.848691	-0.038086	3.508956
189.867652	4149.932626	6.853696	-0.038125	3.512213
190.071944	4157.978874	6.858701	-0.038168	3.515451
190.261230	4165.934143	6.863706	-0.038209	3.518648
190.461025	4174.000351	6.868710	-0.038251	3.521888
190.534277	4181.955736	6.873715	-0.038270	3.525077
190.705977	4190.013993	6.878720	-0.038308	3.528306
191.171268	4198.079566	6.883725	-0.038400	3.531545
191.313768	4206.097159	6.888730	-0.038432	3.534751
191.560329	4214.144080	6.893734	-0.038483	3.537970
191.564401	4222.171847	6.898739	-0.038489	3.541171
191.658649	4230.221362	6.903744	-0.038512	3.544380
191.859788	4238.240483	6.908749	-0.038555	3.547577
191.994829	4246.267107	6.913754	-0.038585	3.550772
192.353781	4254.415061	6.918758	-0.038657	3.554019
192.585480	4262.355693	6.923763	-0.038706	3.557178
192.866049	4270.323544	6.928768	-0.038763	3.560345
193.165900	4278.343735	6.933773	-0.038825	3.563531
193.116891	4286.357213	6.938778	-0.038821	3.566702
193.158995	4294.401988	6.943782	-0.038834	3.569884
193.461001	4302.405091	6.948787	-0.038896	3.573055
193.682624	4310.436292	6.953792	-0.038942	3.576232
193.754665	4318.460975	6.958797	-0.038961	3.579399
193.991823	4326.458740	6.963802	-0.039010	3.582557
194.300813	4334.495023	6.968806	-0.039073	3.585729
194.223095	4342.529694	6.973811	-0.039064	3.588888
194.508658	4350.563791	6.978816	-0.039123	3.592053
194.912054	4358.551393	6.983821	-0.039203	3.595201
195.029969	4366.560855	6.988826	-0.039231	3.598346
195.364607	4374.623420	6.993830	-0.039298	3.601515
195.472423	4382.568869	6.998835	-0.039324	3.604630
195.622825	4390.649167	7.003840	-0.039357	3.607796
195.738382	4398.684752	7.008845	-0.039384	3.610940
195.795640	4406.707487	7.013850	-0.039400	3.614075
196.146199	4414.753587	7.018854	-0.039470	3.617225
196.017968	4422.755245	7.023859	-0.039452	3.620341
196.464915	4430.766358	7.028864	-0.039541	3.623474
196.749244	4438.842401	7.033869	-0.039599	3.626625
196.506851	4446.837430	7.038874	-0.039559	3.629728
197.086421	4454.895227	7.043878	-0.039672	3.632874
197.330864	4462.926130	7.048883	-0.039723	3.635998
197.539319	4470.913372	7.053888	-0.039767	3.639102
197.527738	4478.970887	7.058893	-0.039771	3.642224
197.958537	4486.928624	7.063898	-0.039856	3.645317
198.237633	4495.002901	7.068902	-0.039913	3.648448
198.390252	4503.007142	7.073907	-0.039947	3.651546
198.584693	4511.046171	7.078912	-0.039989	3.654656
198.932110	4519.084295	7.083917	-0.040059	3.657766
198.899588	4527.080343	7.088922	-0.040058	3.660848
199.239413	4535.102039	7.093926	-0.040127	3.663947
199.283310	4543.147144	7.098931	-0.040140	3.667045
199.562715	4551.151770	7.103936	-0.040198	3.670131
199.713839	4559.209148	7.108941	-0.040231	3.673230
199.729520	4567.243295	7.113946	-0.040239	3.676315
200.135343	4575.225965	7.118950	-0.040320	3.679388
200.378413	4583.226173	7.123955	-0.040371	3.682460
200.754962	4591.219555	7.128960	-0.040446	3.685530
201.088658	4599.240531	7.133965	-0.040514	3.688608
201.404505	4607.263803	7.138970	-0.040578	3.691683
201.576316	4615.335140	7.143974	-0.040615	3.694770
201.715098	4623.363072	7.148979	-0.040647	3.697838
202.049580	4631.358103	7.153984	-0.040714	3.700895
202.114894	4639.384567	7.158989	-0.040732	3.703955
202.366687	4647.392637	7.163994	-0.040784	3.707009
202.601438	4655.438080	7.168998	-0.040833	3.710076
202.734314	4663.544436	7.174003	-0.040863	3.713160
202.776286	4671.589346	7.179008	-0.040876	3.716216
203.176836	4679.529329	7.184013	-0.040956	3.719238
203.220949	4687.557741	7.189018	-0.040970	3.722283
203.469807	4695.528768	7.194022	-0.041021	3.725309
203.553899	4703.530743	7.199027	-0.041042	3.728340
203.986991	4711.574459	7.204032	-0.041128	3.731392
204.193103	4719.639920	7.209037	-0.041172	3.734445
204.179015	4727.638891	7.214042	-0.041175	3.737465
204.541157	4735.657482	7.219046	-0.041248	3.740498
204.762265	4743.630137	7.224051	-0.041294	3.743509
205.096723	4751.650440	7.229056	-0.041362	3.746537
205.275879	4759.726741	7.234061	-0.041401	3.749581
205.439797	4767.762448	7.239066	-0.041436	3.752607
205.799892	4775.808571	7.244070	-0.041509	3.755638
205.937871	4783.781666	7.249075	-0.041540	3.758635
206.228436	4791.812740	7.254080	-0.041599	3.761654
206.272278	4799.851114	7.259085	-0.041613	3.764668
206.487752	4807.853952	7.264090	-0.041658	3.767670
206.812814	4815.924313	7.269094	-0.041724	3.770697
206.736660	4823.927539	7.274099	-0.041715	3.773688
206.879488	4831.978393	7.279104	-0.041747	3.776699
207.107439	4839.964602	7.284109	-0.041795	3.779686
207.337265	4847.961310	7.289114	-0.041843	3.782674
207.670708	4856.006107	7.294118	-0.041911	3.785680
207.768723	4864.023476	7.299123	-0.041934	3.788668
208.078548	4872.086864	7.304128	-0.041997	3.791675
208.560153	4880.124941	7.309133	-0.042092	3.794675
208.613643	4888.105377	7.314138	-0.042108	3.797641
208.676816	4896.133586	7.319142	-0.042125	3.800623
208.954827	4904.113633	7.324147	-0.042182	3.803589
208.945447	4912.159549	7.329152	-0.042185	3.806571
209.335591	4920.153448	7.334157	-0.042263	3.809540
209.529954	4928.207148	7.339162	-0.042305	3.812525
209.739811	4936.273127	7.344166	-0.042349	3.815512
209.975432	4944.230798	7.349171	-0.042399	3.818457
210.331993	4952.238637	7.354176	-0.042470	3.821421
210.349797	4960.257559	7.359181	-0.042479	3.824380
210.167286	4968.284638	7.364186	-0.042450	3.827335
210.687184	4976.332799	7.369190	-0.042553	3.830310
210.921022	4984.350797	7.374195	-0.042601	3.833266
211.213092	4992.378651	7.379200	-0.042661	3.836225
211.487905	5000.381497	7.384205	-0.042718	3.839171
211.556163	5008.386707	7.389210	-0.042736	3.842112
212.043244	5016.386973	7.394214	-0.042832	3.845058
212.121074	5024.411758	7.399219	-0.042852	3.848001
212.340676	5032.455449	7.404224	-0.042898	3.850953
212.637565	5040.520833	7.409229	-0.042959	3.853911
212.719861	5048.519653	7.414234	-0.042979	3.856838
213.165085	5056.547717	7.419238	-0.043067	3.859782
213.157934	5064.540606	7.424243	-0.043071	3.862701
213.292038	5072.543097	7.429248	-0.043102	3.865624
213.714455	5080.612535	7.434253	-0.043186	3.868575
213.899293	5088.610972	7.439258	-0.043226	3.871493
214.152926	5096.901811	7.444262	-0.043278	3.874516
214.218254	5104.860666	7.449267	-0.043296	3.877413
214.526268	5112.771501	7.454272	-0.043358	3.880295
214.668788	5120.757213	7.459277	-0.043390	3.883199
214.535564	5128.744448	7.464282	-0.043371	3.886096
215.032628	5136.744399	7.469286	-0.043469	3.889007
215.389567	5144.771617	7.474291	-0.043541	3.891924
215.653828	5152.802907	7.479296	-0.043595	3.894837
215.803440	5160.850545	7.484301	-0.043628	3.897753
216.051364	5168.811154	7.489306	-0.043680	3.900636
216.406166	5176.850093	7.494310	-0.043751	3.903548
216.475224	5184.881186	7.499315	-0.043769	3.906449
216.692445	5192.878754	7.504320	-0.043815	3.909339
216.826279	5200.973170	7.509325	-0.043846	3.912260
216.946040	5208.964317	7.514330	-0.043873	3.915141
217.097080	5217.000616	7.519334	-0.043907	3.918037
217.301441	5224.967350	7.524339	-0.043950	3.920907
217.531161	5232.919643	7.529344	-0.043998	3.923770
217.776603	5241.005745	7.534349	-0.044049	3.926679
217.962909	5249.011255	7.539354	-0.044089	3.929556
218.122403	5257.064958	7.544358	-0.044124	3.932447
218.346112	5265.072730	7.549363	-0.044171	3.935321
218.576016	5273.054765	7.554368	-0.044219	3.938184
218.874982	5281.088233	7.559373	-0.044280	3.941064
218.765032	5289.117775	7.564378	-0.044265	3.943934
219.156760	5297.160451	7.569382	-0.044344	3.946815
219.400962	5305.136663	7.574387	-0.044394	3.949668
219.619681	5313.170730	7.579392	-0.044440	3.952538
219.879296	5321.234196	7.584397	-0.044494	3.955418
219.784560	5329.213494	7.589402	-0.044482	3.958260
220.186846	5337.248748	7.594406	-0.044562	3.961128
220.117743	5345.217329	7.599411	-0.044555	3.963962
220.223697	5353.290573	7.604416	-0.044580	3.966834
220.564013	5361.284098	7.609421	-0.044648	3.969680
220.624238	5369.308806	7.614426	-0.044665	3.972530
221.082141	5377.374658	7.619430	-0.044756	3.975399
221.402649	5385.361236	7.624435	-0.044821	3.978236
221.533708	5393.394943	7.629440	-0.044850	3.981084
221.742134	5401.398301	7.634445	-0.044895	3.983921
221.955743	5409.409873	7.639450	-0.044940	3.986758
222.058877	5417.450793	7.644454	-0.044964	3.989602
222.163543	5425.517768	7.649459	-0.044989	3.992454
222.370261	5433.552373	7.654464	-0.045033	3.995293
222.595140	5441.577814	7.659469	-0.045080	3.998128
222.657901	5449.536507	7.664474	-0.045097	4.000934
222.695527	5457.580842	7.669478	-0.045110	4.003768
222.809536	5465.576080	7.674483	-0.045136	4.006584
223.086514	5473.596499	7.679488	-0.045193	4.009409
223.393368	5481.666714	7.684493	-0.045256	4.012251
223.489872	5489.655886	7.689498	-0.045279	4.015058
223.768370	5497.721138	7.694502	-0.045336	4.017894
223.969098	5505.678021	7.699507	-0.045379	4.020687
224.051713	5513.698158	7.704512	-0.045399	4.023500
224.384628	5521.717742	7.709517	-0.045467	4.026314
224.494939	5529.736464	7.714522	-0.045493	4.029122
224.683288	5537.824510	7.719526	-0.045533	4.031953
225.073747	5545.892861	7.724531	-0.045611	4.034779
225.358136	5553.847184	7.729536	-0.045670	4.037562
225.376900	5561.838757	7.734541	-0.045678	4.040351
225.526539	5569.818806	7.739546	-0.045712	4.043136
225.656200	5577.833030	7.744550	-0.045741	4.045932
225.720886	5585.855524	7.749555	-0.045758	4.048727
225.858999	5593.887777	7.754560	-0.045789	4.051524
226.285965	5601.907623	7.759565	-0.045874	4.054320
226.234275	5609.930985	7.764570	-0.045870	4.057108
226.438468	5617.923477	7.769574	-0.045913	4.059887
226.521960	5625.962365	7.774579	-0.045934	4.062678
226.803175	5633.970130	7.779584	-0.045992	4.065459
227.040391	5642.018588	7.784589	-0.046042	4.068252
227.141656	5650.009524	7.789594	-0.046066	4.071022
227.495332	5658.078147	7.794598	-0.046137	4.073819
227.420260	5666.075321	7.799603	-0.046128	4.076584
227.755524	5674.007740	7.804608	-0.046196	4.079331
228.125588	5682.109762	7.809613	-0.046270	4.082134
228.436908	5690.034302	7.814618	-0.046334	4.084874
228.883889	5698.076804	7.819622	-0.046422	4.087654
229.153457	5706.103648	7.824627	-0.046478	4.090425
229.340428	5714.136465	7.829632	-0.046518	4.093194
229.626427	5722.191942	7.834637	-0.046577	4.095971
229.697089	5730.183919	7.839642	-0.046595	4.098721
229.960443	5738.242249	7.844646	-0.046649	4.101495
230.114013	5746.199315	7.849651	-0.046683	4.104230
230.152125	5754.277007	7.854656	-0.046696	4.107004
230.669723	5762.293424	7.859661	-0.046798	4.109760
230.564851	5770.301738	7.864666	-0.046783	4.112505
230.798398	5778.373264	7.869670	-0.046832	4.115273
231.132340	5786.346366	7.874675	-0.046900	4.118007
231.490635	5794.367851	7.879680	-0.046972	4.120756
231.694482	5802.369312	7.884685	-0.047015	4.123494
231.588534	5810.378051	7.889690	-0.047001	4.126229
232.072899	5818.405966	7.894694	-0.047096	4.128976
232.098519	5826.437250	7.899699	-0.047106	4.131717
232.261244	5834.481001	7.904704	-0.047142	4.134462
232.472898	5842.542221	7.909709	-0.047187	4.137211
232.609233	5850.506037	7.914714	-0.047218	4.139925
232.855496	5858.552123	7.919718	-0.047269	4.142666
233.027942	5866.528114	7.924723	-0.047306	4.145381
233.188858	5874.572289	7.929728	-0.047342	4.148117
233.426332	5882.584323	7.934733	-0.047391	4.150841
233.518343	5890.636973	7.939738	-0.047414	4.153575
233.814981	5898.684464	7.944742	-0.047474	4.156308
234.073739	5906.640978	7.949747	-0.047528	4.159008
234.198699	5914.666192	7.954752	-0.047556	4.161728
234.482152	5922.640781	7.959757	-0.047614	4.164430
234.693886	5930.694095	7.964762	-0.047659	4.167157
234.897290	5938.687461	7.969766	-0.047702	4.169862
235.020206	5946.787608	7.974771	-0.047731	4.172600
235.217635	5954.721478	7.979776	-0.047773	4.175281
235.490052	5962.795138	7.984781	-0.047829	4.178008
235.637486	5970.768853	7.989786	-0.047862	4.180698
235.714679	5978.818560	7.994790	-0.047881	4.183411
235.999771	5986.811402	7.999795	-0.047940	4.186106
236.249968	5994.826377	8.004800	-0.047992	4.188806
236.470699	6002.839185	8.009805	-0.048038	4.191503
236.457989	6010.975904	8.014810	-0.048041	4.194237
236.696386	6018.994072	8.019814	-0.048091	4.196933
236.790872	6026.930668	8.024819	-0.048114	4.199598
237.022655	6034.922228	8.029824	-0.048162	4.202281
237.350990	6042.895623	8.034829	-0.048229	4.204957
237.330106	6050.934928	8.039834	-0.048230	4.207650
237.564025	6058.922442	8.044838	-0.048279	4.210327
237.828765	6066.988916	8.049843	-0.048334	4.213028
238.151430	6074.988016	8.054848	-0.048399	4.215706
238.309878	6083.018575	8.059853	-0.048434	4.218391
238.652799	6091.001343	8.064858	-0.048503	4.221060
239.040610	6099.017981	8.069862	-0.048581	4.223739
238.843182	6107.055475	8.074867	-0.048549	4.226417
239.313529	6115.038967	8.079872	-0.048642	4.229083
239.483998	6123.130750	8.084877	-0.048679	4.231779
239.458564	6131.145000	8.089882	-0.048680	4.234447
239.817814	6139.193164	8.094886	-0.048752	4.237127
240.094304	6147.121078	8.099891	-0.048809	4.239766
240.241166	6155.160959	8.104896	-0.048842	4.242438
240.360733	6163.177553	8.109901	-0.048869	4.245101
240.653629	6171.178612	8.114906	-0.048929	4.247758
240.833543	6179.199103	8.119910	-0.048968	4.250419
241.181941	6187.256084	8.124915	-0.049038	4.253092
241.335968	6195.307325	8.129920	-0.049072	4.255760
241.477252	6203.316840	8.134925	-0.049104	4.258412
241.447209	6211.300882	8.139930	-0.049104	4.261053
241.647116	6219.342583	8.144934	-0.049146	4.263713
241.940337	6227.355838	8.149939	-0.049206	4.266363
241.995744	6235.342335	8.154944	-0.049222	4.269000
242.280706	6243.424628	8.159949	-0.049280	4.271669
242.383281	6251.445574	8.164954	-0.049305	4.274314
242.693011	6259.487311	8.169958	-0.049368	4.276967
242.864970	6267.437951	8.174963	-0.049405	4.279586
242.972577	6275.495676	8.179968	-0.049431	4.282239
243.037503	6283.464522	8.184973	-0.049448	4.284861
243.270459	6291.450445	8.189978	-0.049497	4.287488
243.607169	6299.508325	8.194982	-0.049565	4.290137
243.661748	6307.537012	8.199987	-0.049580	4.292773
243.904899	6315.573916	8.204992	-0.049631	4.295412
244.095090	6323.584701	8.209997	-0.049672	4.298040
244.215920	6331.569649	8.215002	-0.049700	4.300658
244.357374	6339.627714	8.220006	-0.049731	4.303298
244.501202	6347.591502	8.225011	-0.049763	4.305905
244.733453	6355.636517	8.230016	-0.049812	4.308538
244.996077	6363.663914	8.235021	-0.049866	4.311164
244.880895	6371.683513	8.240026	-0.049850	4.313783
245.217468	6379.750812	8.245030	-0.049918	4.316419
245.361872	6387.692340	8.250035	-0.049950	4.319012
245.562003	6395.715099	8.255040	-0.049993	4.321629
245.693788	6403.713579	8.260045	-0.050023	4.324237
245.913489	6411.743887	8.265050	-0.050069	4.326854
246.214867	6419.754445	8.270054	-0.050131	4.329463
246.104325	6427.840769	8.275059	-0.050115	4.332093
246.353926	6435.794050	8.280064	-0.050167	4.334680
246.621897	6443.910425	8.285069	-0.050222	4.337318
246.835093	6451.815576	8.290074	-0.050267	4.339887
246.895512	6459.874779	8.295078	-0.050284	4.342502
247.014078	6467.870338	8.300083	-0.050311	4.345096
247.256139	6475.881847	8.305088	-0.050362	4.347694
247.642050	6483.880092	8.310093	-0.050439	4.350287
247.768441	6491.952793	8.315098	-0.050468	4.352901
248.216250	6500.058207	8.320102	-0.050557	4.355526
248.109544	6507.999262	8.325107	-0.050542	4.358093
248.225541	6515.942838	8.330112	-0.050569	4.360661
248.633129	6524.012571	8.335117	-0.050650	4.363269
248.564419	6531.966142	8.340122	-0.050643	4.365836
248.682317	6540.040167	8.345126	-0.050670	4.368441
248.968349	6548.011508	8.350131	-0.050729	4.371012
249.239876	6556.032505	8.355136	-0.050785	4.373598
249.255994	6564.084060	8.360141	-0.050793	4.376190
249.311176	6572.060165	8.365146	-0.050809	4.378757
249.811860	6580.081141	8.370150	-0.050907	4.381339
249.950770	6588.110098	8.375155	-0.050938	4.383921
250.094080	6596.132114	8.380160	-0.050971	4.386498
250.456516	6604.160257	8.385165	-0.051043	4.389077
250.416180	6612.173387	8.390170	-0.051041	4.391648
250.633493	6620.234889	8.395174	-0.051087	4.394234
250.941668	6628.234535	8.400179	-0.051150	4.396799
251.153238	6636.170252	8.405184	-0.051194	4.399341
251.357883	6644.280526	8.410189	-0.051238	4.401938
251.435528	6652.215986	8.415194	-0.051258	4.404477
251.660433	6660.256466	8.420198	-0.051305	4.407049
251.691048	6668.297715	8.425203	-0.051316	4.409618
251.836298	6676.311719	8.430208	-0.051348	4.412178
252.223474	6684.374979	8.435213	-0.051426	4.414753
252.270042	6692.379309	8.440218	-0.051440	4.417306
252.563381	6700.366299	8.445222	-0.051500	4.419853
252.640598	6708.454067	8.450227	-0.051520	4.422430
253.068364	6716.357526	8.455232	-0.051605	4.424948
253.354376	6724.439271	8.460237	-0.051663	4.427521
253.394783	6732.437690	8.465242	-0.051676	4.430065
253.689226	6740.513154	8.470246	-0.051736	4.432633
253.736633	6748.532618	8.475251	-0.051750	4.435180
253.964682	6756.527932	8.480256	-0.051798	4.437720
254.357530	6764.542657	8.485261	-0.051877	4.440264
254.564000	6772.550582	8.490266	-0.051920	4.442804
254.587238	6780.514090	8.495270	-0.051930	4.445328
254.554999	6788.556729	8.500275	-0.051929	4.447875
254.894688	6796.572129	8.505280	-0.051998	4.450414
254.988626	6804.635462	8.510285	-0.052021	4.452965
255.028294	6812.620107	8.515290	-0.052034	4.455490
255.180498	6820.630823	8.520294	-0.052067	4.458022
255.389041	6828.622824	8.525299	-0.052112	4.460546
255.428149	6836.647913	8.530304	-0.052124	4.463080
255.925906	6844.666982	8.535309	-0.052222	4.465611
255.987502	6852.704071	8.540314	-0.052239	4.468145
256.183990	6860.704794	8.545318	-0.052281	4.470667
256.324746	6868.745362	8.550323	-0.052313	4.473199
256.605354	6876.784277	8.555328	-0.052370	4.475730
256.865104	6884.764517	8.560333	-0.052424	4.478241
256.913491	6892.758200	8.565338	-0.052438	4.480755
257.102573	6900.764106	8.570343	-0.052479	4.483271
257.260942	6908.779829	8.575347	-0.052514	4.485788
257.306981	6916.793110	8.580352	-0.052527	4.488303
257.886572	6924.852331	8.585357	-0.052641	4.490833
257.789197	6932.866967	8.590362	-0.052628	4.493345
258.112537	6940.897722	8.595367	-0.052694	4.495862
258.340662	6948.878989	8.600371	-0.052741	4.498362
258.329186	6956.887525	8.605376	-0.052745	4.500868
258.586411	6964.930538	8.610381	-0.052798	4.503384
258.810036	6972.872504	8.615386	-0.052845	4.505868
259.047817	6980.961784	8.620391	-0.052894	4.508395
259.287096	6988.989691	8.625395	-0.052944	4.510903
259.451902	6997.037656	8.630400	-0.052980	4.513415
259.626484	7005.092120	8.635405	-0.053018	4.515927
259.760097	7013.010143	8.640410	-0.053048	4.518396
260.177240	7021.022112	8.645415	-0.053131	4.520893
260.284207	7028.978256	8.650419	-0.053157	4.523370
260.638275	7036.994662	8.655424	-0.053228	4.525866
260.970108	7045.084030	8.660429	-0.053295	4.528383
260.812777	7053.042885	8.665434	-0.053271	4.530856
261.187322	7061.069788	8.670439	-0.053346	4.533351
261.452037	7069.105804	8.675443	-0.053401	4.535847
261.628718	7077.136689	8.680448	-0.053439	4.538339
261.849779	7085.152749	8.685453	-0.053486	4.540826
262.085718	7093.147046	8.690458	-0.053535	4.543304
262.202475	7101.150303	8.695463	-0.053562	4.545784
262.081333	7109.226428	8.700467	-0.053545	4.548285
262.335689	7117.168422	8.705472	-0.053597	4.550743
262.750040	7125.297027	8.710477	-0.053680	4.553258
262.706788	7133.259987	8.715482	-0.053677	4.555720
262.822321	7141.298545	8.720487	-0.053704	4.558204
263.185107	7149.256940	8.725491	-0.053777	4.560662
263.090101	7157.268479	8.730496	-0.053765	4.563134
263.301288	7165.305900	8.735501	-0.053809	4.565614
263.318175	7173.324895	8.740506	-0.053818	4.568086
263.775359	7181.296733	8.745511	-0.053908	4.570543
263.687160	7189.369301	8.750515	-0.053897	4.573029
264.003078	7197.357354	8.755520	-0.053961	4.575488
264.339262	7205.431020	8.760525	-0.054029	4.577971
264.464107	7213.413975	8.765530	-0.054058	4.580426
264.562315	7221.439911	8.770535	-0.054082	4.582892
264.804641	7229.450793	8.775539	-0.054132	4.585353
265.091893	7237.447744	8.780544	-0.054191	4.587808
265.338377	7245.535634	8.785549	-0.054242	4.590289
265.586910	7253.539402	8.790554	-0.054294	4.592743
265.963002	7261.543487	8.795559	-0.054369	4.595196
265.831209	7269.593677	8.800563	-0.054350	4.597662
265.805381	7277.518642	8.805568	-0.054350	4.600088
266.358438	7285.583906	8.810573	-0.054459	4.602556
266.426481	7293.537920	8.815578	-0.054477	4.604988
266.539524	7301.599417	8.820583	-0.054503	4.607452
266.658346	7309.574305	8.825587	-0.054531	4.609888
266.751571	7317.616845	8.830592	-0.054553	4.612343
267.237878	7325.651051	8.835597	-0.054649	4.614795
267.258272	7333.701165	8.840602	-0.054658	4.617250
267.254945	7341.664354	8.845607	-0.054663	4.619677
267.569593	7349.708294	8.850611	-0.054727	4.622128
267.730339	7357.636271	8.855616	-0.054762	4.624542
267.995103	7365.718545	8.860621	-0.054817	4.627001
268.155916	7373.732047	8.865626	-0.054852	4.629439
268.197508	7381.788518	8.870631	-0.054865	4.631888
268.460812	7389.816072	8.875635	-0.054920	4.634327
268.706543	7397.804717	8.880640	-0.054971	4.636753
268.918554	7405.801644	8.885645	-0.055016	4.639180
268.911605	7413.826725	8.890650	-0.055020	4.641614
269.259242	7421.801822	8.895655	-0.055090	4.644032
269.406152	7429.880336	8.900659	-0.055123	4.646480
269.254585	7437.846392	8.905664	-0.055100	4.648893
269.610594	7445.914796	8.910669	-0.055171	4.651335
269.641932	7453.869408	8.915674	-0.055182	4.653742
269.785877	7461.896872	8.920679	-0.055215	4.656169
270.157674	7469.915303	8.925683	-0.055289	4.658592
270.113227	7477.890344	8.930688	-0.055286	4.661001
270.290112	7485.967955	8.935693	-0.055325	4.663440
270.394239	7493.934587	8.940698	-0.055349	4.665844
270.791094	7501.979594	8.945703	-0.055428	4.668269
270.876094	7510.029103	8.950707	-0.055450	4.670696
270.929056	7518.055688	8.955712	-0.055465	4.673114
271.261358	7526.100731	8.960717	-0.055532	4.675536
271.417435	7534.075231	8.965722	-0.055567	4.677936
271.456297	7542.028168	8.970727	-0.055579	4.680329
271.752077	7550.088813	8.975731	-0.055640	4.682752
271.994991	7558.028671	8.980736	-0.055690	4.685137
272.145950	7566.133137	8.985741	-0.055724	4.687571
272.075600	7574.016524	8.990746	-0.055716	4.689938
272.440858	7582.114434	8.995751	-0.055789	4.692367
272.368535	7590.112133	9.000755	-0.055781	4.694765
272.409013	7598.164848	9.005760	-0.055794	4.697179
272.769342	7606.144186	9.010765	-0.055866	4.699569
273.106409	7614.152561	9.015770	-0.055934	4.701966
272.989534	7622.124601	9.020775	-0.055918	4.704352
273.102085	7630.207137	9.025779	-0.055944	4.706769
273.496152	7638.195177	9.030784	-0.056023	4.709156
273.656126	7646.261499	9.035789	-0.056058	4.711566
273.729883	7654.274724	9.040794	-0.056077	4.713959
274.193872	7662.323115	9.045799	-0.056169	4.716360
274.389767	7670.306105	9.050803	-0.056211	4.718741
274.294153	7678.236807	9.055808	-0.056198	4.721107
274.557881	7686.315618	9.060813	-0.056253	4.723514
274.643574	7694.331768	9.065818	-0.056274	4.725901
274.816415	7702.344570	9.070823	-0.056312	4.728287
274.915016	7710.453014	9.075827	-0.056335	4.730699
275.130297	7718.413675	9.080832	-0.056381	4.733066
275.320713	7726.472665	9.085837	-0.056422	4.735462
275.514721	7734.470700	9.090842	-0.056463	4.737837
275.802080	7742.437137	9.095847	-0.056522	4.740202
276.094478	7750.498206	9.100851	-0.056582	4.742594
276.022987	7758.437965	9.105856	-0.056574	4.744950
276.360751	7766.546812	9.110861	-0.056642	4.747353
276.617065	7774.468171	9.115866	-0.056695	4.749700
276.475829	7782.491760	9.120871	-0.056674	4.752077
276.920064	7790.630309	9.125875	-0.056762	4.754485
277.147969	7798.584583	9.130880	-0.056810	4.756839
277.372421	7806.552346	9.135885	-0.056857	4.759194
277.333072	7814.590274	9.140890	-0.056855	4.761571
277.485806	7822.569341	9.145895	-0.056889	4.763928
277.861286	7830.628507	9.150899	-0.056964	4.766307
277.844649	7838.599532	9.155904	-0.056966	4.768660
277.913142	7846.657220	9.160909	-0.056985	4.771037
278.155727	7854.631494	9.165914	-0.057035	4.773387
278.476539	7862.666051	9.170919	-0.057100	4.775754
278.510273	7870.699359	9.175923	-0.057112	4.778121
278.824433	7878.665635	9.180928	-0.057176	4.780465
279.258280	7886.733288	9.185933	-0.057262	4.782837
279.210490	7894.690394	9.190938	-0.057258	4.785178
279.442116	7902.756696	9.195943	-0.057307	4.787549
279.477017	7910.711311	9.200947	-0.057318	4.789886
279.520918	7918.789052	9.205952	-0.057332	4.792259
279.702602	7926.782663	9.210957	-0.057371	4.794604
279.886426	7934.861184	9.215962	-0.057411	4.796974
280.126459	7942.756260	9.220967	-0.057461	4.799288
280.241256	7950.848067	9.225971	-0.057488	4.801660
280.428115	7958.785293	9.230976	-0.057528	4.803985
280.683056	7966.927028	9.235981	-0.057580	4.806368
280.760407	7974.856421	9.240986	-0.057600	4.808688
281.006356	7982.902615	9.245991	-0.057651	4.811041
281.252770	7990.426384	9.250995	-0.057702	4.813240
281.326613	7995.091839	9.256000	-0.057719	4.814603

281.525163	7997.540714	9.261005	-0.057758	4.815318
281.639886	7998.714833	9.266010	-0.057780	4.815660
281.825242	7999.723638	9.271015	-0.057815	4.815954
281.844897	7999.690883	9.276019	-0.057819	4.815944
282.115453	7999.680851	9.281024	-0.057870	4.815940
282.380164	7999.724140	9.286029	-0.057919	4.815951
282.422535	7999.675770	9.291034	-0.057927	4.815937
282.429796	7999.703695	9.296039	-0.057929	4.815945
282.672685	7999.866263	9.301043	-0.057974	4.815991
282.631483	8000.057863	9.306048	-0.057967	4.816047
282.529481	7999.948098	9.311053	-0.057948	4.816016
282.636225	7999.951119	9.316058	-0.057968	4.816016
282.804891	7999.905044	9.321063	-0.057999	4.816002
282.832431	7999.842513	9.326067	-0.058004	4.815983
282.662955	8000.043535	9.331072	-0.057973	4.816043
282.904489	7999.979552	9.336077	-0.058018	4.816023
282.832363	8000.241116	9.341082	-0.058005	4.816100
282.746505	7999.964949	9.346087	-0.057989	4.816020
282.969331	7999.879255	9.351091	-0.058030	4.815993
282.945912	8000.042329	9.356096	-0.058026	4.816041
282.953382	7999.823425	9.361101	-0.058028	4.815977
283.017549	7999.880167	9.366106	-0.058040	4.815993
283.107097	7999.841203	9.371111	-0.058057	4.815981
283.007289	7999.995408	9.376115	-0.058038	4.816027
283.028584	8000.078085	9.381120	-0.058042	4.816051
283.356114	7999.875685	9.386125	-0.058103	4.815990
283.265100	7999.979829	9.391130	-0.058087	4.816021
283.107187	7999.923542	9.396135	-0.058057	4.816005
283.307169	7999.889791	9.401139	-0.058095	4.815995
283.251176	7999.995640	9.406144	-0.058084	4.816026
283.455364	7999.920292	9.411149	-0.058122	4.816003
283.390573	8000.039873	9.416154	-0.058111	4.816038
283.352521	7999.907760	9.421159	-0.058104	4.816000
283.374744	7999.882531	9.426163	-0.058108	4.815992
283.415174	7999.984791	9.431168	-0.058116	4.816022
283.389251	7999.860379	9.436173	-0.058111	4.815985
283.400212	7999.833876	9.441178	-0.058113	4.815978
283.408888	7999.891748	9.446183	-0.058115	4.815995
283.668093	7999.928530	9.451187	-0.058163	4.816004
283.780148	7999.829066	9.456192	-0.058184	4.815974
283.739215	7999.809100	9.461197	-0.058176	4.815969
283.590980	8000.101340	9.466202	-0.058149	4.816055
283.652674	8000.153766	9.471207	-0.058161	4.816070
283.759493	8000.135418	9.476211	-0.058181	4.816064
283.747818	8000.259173	9.481216	-0.058179	4.816100
283.702307	7999.997624	9.486221	-0.058170	4.816024
283.764745	8000.054338	9.491226	-0.058182	4.816040
283.716447	8000.027825	9.496231	-0.058173	4.816033
283.750544	7999.880995	9.501235	-0.058180	4.815990
283.669907	7999.969300	9.506240	-0.058165	4.816016
283.832152	7999.991497	9.511245	-0.058195	4.816021
283.795110	7999.967327	9.516250	-0.058188	4.816015
283.899093	8000.115625	9.521255	-0.058208	4.816057
284.051497	7999.737998	9.526259	-0.058236	4.815946
283.840178	8000.104960	9.531264	-0.058197	4.816054
284.221421	7999.750729	9.536269	-0.058268	4.815949
284.099237	7999.965438	9.541274	-0.058246	4.816012
284.023863	8000.137189	9.546279	-0.058232	4.816063
284.025693	7999.875433	9.551283	-0.058232	4.815986
284.144313	8000.130856	9.556288	-0.058254	4.816060
283.936700	7999.865290	9.561293	-0.058216	4.815984
283.837147	8000.103920	9.566298	-0.058197	4.816054
283.945976	8000.042866	9.571303	-0.058218	4.816036
284.041149	8000.178182	9.576307	-0.058236	4.816075
284.098835	8000.208095	9.581312	-0.058247	4.816083
284.150603	8000.004949	9.586317	-0.058256	4.816024
284.118655	8000.179628	9.591322	-0.058251	4.816075
284.050024	7999.981772	9.596327	-0.058238	4.816017
284.183710	8000.011999	9.601331	-0.058263	4.816025
284.010274	8000.228984	9.606336	-0.058231	4.816090
284.204844	7999.967527	9.611341	-0.058267	4.816012
284.215601	8000.194275	9.616346	-0.058269	4.816079
284.331249	8000.198528	9.621351	-0.058291	4.816079
284.373747	8000.068945	9.626355	-0.058299	4.816041
284.310135	7999.986587	9.631360	-0.058287	4.816017
284.490278	7999.827452	9.636365	-0.058321	4.815970
284.504040	8000.011511	9.641370	-0.058323	4.816024
284.370022	8000.066788	9.646375	-0.058299	4.816040
284.342730	8000.079127	9.651379	-0.058294	4.816044
284.207121	8000.117278	9.656384	-0.058269	4.816056
284.444257	7999.850184	9.661389	-0.058313	4.815977
284.364179	8000.003683	9.666394	-0.058298	4.816022
284.374119	7999.992122	9.671399	-0.058300	4.816019
284.703307	8000.041935	9.676403	-0.058361	4.816031
284.614292	8000.368389	9.681408	-0.058345	4.816127
284.461558	7999.895438	9.686413	-0.058317	4.815990
284.606486	8000.022043	9.691418	-0.058344	4.816026
284.375948	8000.041370	9.696423	-0.058301	4.816033
284.576900	8000.000157	9.701427	-0.058338	4.816020
284.649473	8000.170328	9.706432	-0.058352	4.816069
284.567578	7999.869644	9.711437	-0.058337	4.815982
284.554701	7999.850187	9.716442	-0.058335	4.815976
284.527020	7999.988611	9.721447	-0.058330	4.816017
284.522384	8000.039831	9.726451	-0.058329	4.816032
284.447851	8000.068408	9.731456	-0.058315	4.816040
284.431879	8000.169646	9.736461	-0.058312	4.816070
284.567926	8000.034284	9.741466	-0.058338	4.816030
284.811833	8000.078272	9.746471	-0.058383	4.816041
284.656543	7999.871358	9.751475	-0.058354	4.815982
284.627567	8000.050366	9.756480	-0.058349	4.816034
284.582251	8000.010015	9.761485	-0.058341	4.816023
284.705915	8000.178979	9.766490	-0.058364	4.816071
284.725061	7999.962414	9.771495	-0.058368	4.816008
284.866497	7999.881649	9.776499	-0.058394	4.815984
284.793166	7999.986117	9.781504	-0.058381	4.816015
284.817900	7999.864760	9.786509	-0.058385	4.815979
284.936149	8000.024007	9.791514	-0.058408	4.816025
284.879557	8000.083899	9.796519	-0.058397	4.816043
284.965700	7999.970070	9.801523	-0.058413	4.816009
284.839095	7999.995562	9.806528	-0.058390	4.816017
284.832075	7999.844774	9.811533	-0.058389	4.815973
284.660892	7999.852358	9.816538	-0.058357	4.815976
284.879234	7999.864891	9.821543	-0.058398	4.815979
285.007362	7999.851205	9.826547	-0.058422	4.815974
285.013762	7999.870568	9.831552	-0.058423	4.815980
284.741374	7999.766246	9.836557	-0.058372	4.815951
284.998424	7999.902371	9.841562	-0.058420	4.815989
284.792998	8000.007642	9.846567	-0.058382	4.816021
284.783432	7999.872837	9.851571	-0.058381	4.815981
284.714903	8000.005176	9.856576	-0.058368	4.816020
285.006184	7999.979499	9.861581	-0.058422	4.816011
284.837935	8000.017056	9.866586	-0.058391	4.816023
284.852766	8000.007721	9.871591	-0.058394	4.816020
284.920878	7999.850820	9.876595	-0.058407	4.815974
285.007257	8000.125965	9.881600	-0.058423	4.816054
284.844212	7999.784265	9.886605	-0.058393	4.815955
284.890888	7999.958238	9.891610	-0.058402	4.816006
284.820330	7999.831941	9.896615	-0.058388	4.815969
284.879490	7999.994387	9.901619	-0.058400	4.816016
284.829508	8000.224308	9.906624	-0.058391	4.816084
285.006830	7999.898417	9.911629	-0.058424	4.815988
285.043427	7999.935427	9.916634	-0.058431	4.815998
285.072951	7999.919947	9.921639	-0.058436	4.815994
284.930636	7999.905615	9.926643	-0.058410	4.815990
285.147362	8000.088028	9.931648	-0.058450	4.816042
284.915754	7999.836979	9.936653	-0.058407	4.815970
284.890524	7999.963694	9.941658	-0.058403	4.816007
285.134516	7999.870903	9.946663	-0.058448	4.815979
285.155459	7999.829621	9.951667	-0.058452	4.815967
284.927538	8000.037068	9.956672	-0.058410	4.816029
285.181312	7999.814086	9.961677	-0.058457	4.815962
285.170565	8000.054338	9.966682	-0.058456	4.816032
285.047415	7999.759313	9.971687	-0.058433	4.815947
285.078227	7999.854991	9.976691	-0.058438	4.815975
284.957606	7999.847465	9.981696	-0.058416	4.815973
285.058356	7999.811909	9.986701	-0.058435	4.815962
284.947125	7999.913551	9.991706	-0.058414	4.815992
285.101525	7999.976214	9.996711	-0.058443	4.816010
285.047052	7999.857689	10.001715	-0.058433	4.815976
285.034265	7999.984631	10.006720	-0.058431	4.816013
285.130257	7999.773739	10.011725	-0.058449	4.815951
285.282415	7999.848115	10.016730	-0.058477	4.815971
285.229952	7999.948690	10.021735	-0.058468	4.816001
285.293004	7999.927409	10.026739	-0.058480	4.815995
285.337775	8000.129134	10.031744	-0.058488	4.816053
285.375734	7999.979163	10.036749	-0.058495	4.816009
285.297179	8000.011941	10.041754	-0.058481	4.816019
285.294241	7999.989458	10.046759	-0.058480	4.816013
285.502554	7999.903498	10.051763	-0.058519	4.815986
285.312285	7999.974850	10.056768	-0.058484	4.816008
285.453466	7999.779739	10.061773	-0.058510	4.815951
285.287563	7999.947709	10.066778	-0.058480	4.816000
285.187897	8000.001475	10.071783	-0.058461	4.816017
285.310311	7999.891511	10.076787	-0.058484	4.815984
285.225659	8000.049205	10.081792	-0.058469	4.816030
285.199900	7999.930133	10.086797	-0.058464	4.815996
285.333755	7999.942198	10.091802	-0.058489	4.815999
285.355562	7999.983214	10.096807	-0.058493	4.816010
285.404135	7999.952051	10.101811	-0.058502	4.816001
285.399473	7999.853667	10.106816	-0.058501	4.815972
285.428982	7999.947184	10.111821	-0.058507	4.816000
285.472622	7999.962951	10.116826	-0.058515	4.816004
285.378832	7999.977285	10.121831	-0.058498	4.816009
285.611660	7999.877879	10.126835	-0.058541	4.815978
285.419535	8000.000491	10.131840	-0.058506	4.816015
285.425703	7999.891617	10.136845	-0.058507	4.815983
285.539655	8000.110632	10.141850	-0.058529	4.816047
285.336171	8000.042823	10.146855	-0.058491	4.816028
285.544955	7999.852147	10.151859	-0.058530	4.815971
285.224931	8000.109213	10.156864	-0.058470	4.816048
285.399202	7999.951037	10.161869	-0.058503	4.816001
285.606531	7999.951616	10.166874	-0.058542	4.816000
285.402388	7999.937227	10.171879	-0.058504	4.815997
285.500244	7999.747739	10.176883	-0.058522	4.815941
285.644480	8000.064548	10.181888	-0.058549	4.816033
285.534863	8000.034780	10.186893	-0.058529	4.816025
285.644474	7999.862603	10.191898	-0.058549	4.815974
285.594132	7999.910855	10.196903	-0.058540	4.815988
285.500820	7999.893140	10.201907	-0.058523	4.815983
285.366839	7999.840489	10.206912	-0.058498	4.815969
285.581660	8000.043172	10.211917	-0.058538	4.816027
285.418557	7999.957932	10.216922	-0.058508	4.816003
285.537539	8000.094756	10.221927	-0.058530	4.816042
285.519714	7999.872171	10.226931	-0.058527	4.815977
285.608364	7999.850287	10.231936	-0.058543	4.815970
285.473740	8000.041268	10.236941	-0.058519	4.816027
285.377521	8000.075861	10.241946	-0.058501	4.816037
285.544570	8000.102424	10.246951	-0.058532	4.816044
285.565430	7999.957483	10.251955	-0.058536	4.816002
285.334493	8000.083663	10.256960	-0.058493	4.816040
285.435182	7999.990401	10.261965	-0.058512	4.816012
285.484248	7999.855593	10.266970	-0.058521	4.815972
285.393811	7999.937310	10.271975	-0.058505	4.815997
285.585242	7999.981413	10.276979	-0.058540	4.816009
285.631195	8000.114771	10.281984	-0.058549	4.816047
285.711761	7999.969848	10.286989	-0.058564	4.816005
285.698353	7999.997400	10.291994	-0.058562	4.816013
285.667778	7999.981895	10.296999	-0.058556	4.816008
285.696909	7999.854203	10.302003	-0.058562	4.815971
285.346545	7999.999582	10.307008	-0.058497	4.816015
285.666028	7999.842979	10.312013	-0.058556	4.815968
285.755704	8000.051935	10.317018	-0.058573	4.816028
285.622813	7999.965107	10.322023	-0.058548	4.816004
285.671681	7999.864490	10.327027	-0.058558	4.815974
285.679129	7999.853952	10.332032	-0.058559	4.815971
285.820266	7999.843709	10.337037	-0.058585	4.815967
285.635180	7999.781579	10.342042	-0.058551	4.815950
285.728463	7999.873052	10.347047	-0.058569	4.815976
285.887661	7999.852452	10.352051	-0.058598	4.815969
285.676920	7999.971519	10.357056	-0.058559	4.816005
285.757625	7999.876824	10.362061	-0.058574	4.815977
285.881578	8000.000915	10.367066	-0.058598	4.816013
285.699923	8000.095934	10.372071	-0.058564	4.816041
285.535824	7999.853589	10.377075	-0.058533	4.815971
285.731296	7999.962951	10.382080	-0.058570	4.816002
285.777826	7999.759705	10.387085	-0.058579	4.815943
285.674185	7999.848662	10.392090	-0.058560	4.815969
285.581667	7999.963469	10.397095	-0.058543	4.816003
285.693493	7999.839420	10.402099	-0.058563	4.815966
285.797446	7999.966352	10.407104	-0.058583	4.816003
285.928482	7999.862956	10.412109	-0.058607	4.815972
286.017787	7999.856044	10.417114	-0.058624	4.815970
285.797489	7999.996310	10.422119	-0.058583	4.816012
285.894499	7999.779021	10.427123	-0.058601	4.815948
285.824454	7999.947668	10.432128	-0.058589	4.815997
286.081009	7999.895713	10.437133	-0.058636	4.815981
286.092649	8000.012417	10.442138	-0.058639	4.816015
285.899341	8000.053793	10.447143	-0.058603	4.816028
286.069586	7999.998129	10.452147	-0.058635	4.816011
286.064680	8000.156210	10.457152	-0.058634	4.816057
285.888025	7999.975613	10.462157	-0.058601	4.816005
286.053888	8000.109017	10.467162	-0.058632	4.816043
285.892323	7999.936176	10.472167	-0.058602	4.815994
286.068024	7999.945798	10.477171	-0.058635	4.815995
285.863455	8000.120547	10.482176	-0.058597	4.816048
285.853306	7999.980384	10.487181	-0.058595	4.816007
285.975297	7999.901401	10.492186	-0.058618	4.815983
285.754232	7999.976467	10.497191	-0.058577	4.816006
286.040977	7999.757289	10.502195	-0.058631	4.815941
286.030346	8000.001821	10.507200	-0.058629	4.816012
286.145713	7999.959051	10.512205	-0.058650	4.815999
286.230089	7999.923197	10.517210	-0.058666	4.815988
286.048951	7999.848314	10.522215	-0.058633	4.815967
285.952978	7999.954510	10.527219	-0.058615	4.815999
285.908459	7999.933408	10.532224	-0.058607	4.815993
285.922883	7999.853536	10.537229	-0.058609	4.815969
285.948433	7999.955532	10.542234	-0.058614	4.815999
285.772777	7999.863651	10.547239	-0.058582	4.815973
285.912765	7999.859799	10.552243	-0.058608	4.815971
285.946780	7999.968361	10.557248	-0.058614	4.816003
286.018144	7999.967535	10.562253	-0.058628	4.816002
285.970613	7999.886535	10.567258	-0.058619	4.815979
286.036869	8000.065145	10.572263	-0.058632	4.816030
286.242614	8000.009059	10.577267	-0.058670	4.816013
286.044628	7999.979820	10.582272	-0.058633	4.816005
286.214525	7999.971170	10.587277	-0.058665	4.816002
286.220345	8000.014033	10.592282	-0.058666	4.816015
286.078550	7999.948414	10.597287	-0.058640	4.815996
286.096511	7999.943410	10.602291	-0.058643	4.815995
285.932292	8000.154159	10.607296	-0.058613	4.816057
286.083900	7999.959234	10.612301	-0.058641	4.815999
286.253445	7999.946303	10.617306	-0.058673	4.815995
286.147031	7999.966819	10.622311	-0.058653	4.816001
286.088681	7999.863181	10.627315	-0.058643	4.815971
286.027991	8000.045892	10.632320	-0.058631	4.816025
286.129032	8000.039194	10.637325	-0.058650	4.816022
285.980868	7999.869803	10.642330	-0.058623	4.815974
285.904266	7999.980626	10.647335	-0.058609	4.816006
286.036182	7999.940295	10.652339	-0.058633	4.815994
285.977345	8000.147619	10.657344	-0.058623	4.816055
286.051429	7999.945939	10.662349	-0.058637	4.815995
286.046531	8000.027078	10.667354	-0.058636	4.816019
286.049148	8000.004696	10.672359	-0.058636	4.816013
286.164867	8000.011089	10.677363	-0.058658	4.816014
286.100861	8000.108251	10.682368	-0.058646	4.816043
286.117048	8000.018792	10.687373	-0.058649	4.816016
286.168670	7999.962038	10.692378	-0.058659	4.816000
286.002292	8000.041305	10.697383	-0.058628	4.816024
286.101279	7999.888168	10.702387	-0.058647	4.815978
286.060574	8000.042390	10.707392	-0.058639	4.816024
286.168190	7999.841322	10.712397	-0.058659	4.815964
286.375226	7999.872887	10.717402	-0.058698	4.815972
286.209148	7999.971395	10.722407	-0.058667	4.816002
286.072151	7999.852433	10.727411	-0.058642	4.815968
286.120417	8000.021098	10.732416	-0.058651	4.816017
286.166295	7999.951416	10.737421	-0.058660	4.815996
286.243247	7999.873750	10.742426	-0.058674	4.815973
286.289301	7999.851091	10.747431	-0.058683	4.815966
286.228230	7999.866020	10.752435	-0.058672	4.815971
286.252212	7999.974400	10.757440	-0.058676	4.816003
286.336599	7999.778252	10.762445	-0.058692	4.815945
286.399935	7999.870251	10.767450	-0.058704	4.815971
286.298903	7999.902619	10.772455	-0.058685	4.815981
286.449504	7999.838049	10.777459	-0.058713	4.815962
286.280009	7999.864897	10.782464	-0.058682	4.815971
286.414170	7999.864146	10.787469	-0.058707	4.815970
286.354992	7999.817129	10.792474	-0.058696	4.815956
286.303947	8000.006429	10.797479	-0.058687	4.816012
286.356468	7999.962514	10.802483	-0.058697	4.815999
286.198874	8000.107129	10.807488	-0.058668	4.816042
286.236159	7999.977446	10.812493	-0.058675	4.816004
286.310974	8000.016222	10.817498	-0.058689	4.816015
286.303737	8000.129379	10.822503	-0.058688	4.816048
286.511600	8000.059439	10.827507	-0.058726	4.816026
286.325773	8000.208884	10.832512	-0.058692	4.816071
286.415460	8000.025653	10.837517	-0.058709	4.816017
286.628095	7999.939771	10.842522	-0.058748	4.815990
286.258334	8000.117925	10.847527	-0.058680	4.816045
286.212748	7999.945057	10.852531	-0.058671	4.815994
286.288412	8000.152694	10.857536	-0.058686	4.816054
286.418718	7999.861202	10.862541	-0.058710	4.815969
286.542868	7999.876298	10.867546	-0.058733	4.815972
286.325744	8000.008074	10.872551	-0.058693	4.816012
286.514922	7999.939931	10.877555	-0.058728	4.815991
286.411457	8000.143239	10.882560	-0.058709	4.816051
286.480897	7999.988493	10.887565	-0.058722	4.816005
286.362597	7999.849566	10.892570	-0.058700	4.815966
286.396934	8000.023322	10.897575	-0.058707	4.816016
286.528981	7999.930630	10.902579	-0.058731	4.815988
286.432948	7999.851952	10.907584	-0.058714	4.815966
286.292119	7999.787420	10.912589	-0.058687	4.815948
286.447455	7999.852240	10.917594	-0.058716	4.815966
286.325746	7999.886369	10.922599	-0.058694	4.815976
286.492121	7999.858420	10.927603	-0.058725	4.815967
286.371288	8000.024008	10.932608	-0.058703	4.816016
286.506897	7999.931380	10.937613	-0.058728	4.815989
286.608298	7999.859502	10.942618	-0.058747	4.815967
286.280608	8000.068344	10.947623	-0.058686	4.816030
286.272200	8000.014771	10.952627	-0.058685	4.816014
286.390759	8000.145179	10.957632	-0.058707	4.816052
286.419995	8000.024967	10.962637	-0.058713	4.816016
286.463613	7999.860134	10.967642	-0.058721	4.815968
286.470001	7999.852782	10.972647	-0.058722	4.815966
286.539925	7999.881851	10.977651	-0.058735	4.815974
286.549828	7999.866014	10.982656	-0.058737	4.815969
286.560112	7999.860870	10.987661	-0.058739	4.815968
286.495744	7999.867191	10.992666	-0.058727	4.815970
286.438535	8000.110880	10.997671	-0.058717	4.816041
286.573564	7999.854739	11.002675	-0.058742	4.815966
286.718559	7999.857391	11.007680	-0.058769	4.815966
286.731583	7999.870464	11.012685	-0.058772	4.815970
286.471155	7999.777038	11.017690	-0.058723	4.815944
286.319171	7999.860842	11.022695	-0.058695	4.815969
286.621810	7999.883462	11.027699	-0.058752	4.815974
286.496744	8000.023326	11.032704	-0.058729	4.816015
286.306501	7999.892706	11.037709	-0.058693	4.815978
286.455699	7999.847346	11.042714	-0.058721	4.815964
286.415678	7999.970591	11.047719	-0.058714	4.816000
286.478135	7999.760151	11.052723	-0.058725	4.815939
286.446749	8000.096212	11.057728	-0.058720	4.816037
286.514262	7999.878382	11.062733	-0.058732	4.815973
286.561543	7999.759568	11.067738	-0.058741	4.815938
286.479380	7999.999595	11.072743	-0.058726	4.816009
286.665587	7999.882241	11.077747	-0.058761	4.815973
286.649004	7999.761196	11.082752	-0.058758	4.815938
286.590845	7999.909758	11.087757	-0.058747	4.815982
286.735694	7999.856838	11.092762	-0.058774	4.815966
286.640298	7999.910682	11.097767	-0.058757	4.815982
286.629678	7999.852794	11.102771	-0.058755	4.815965
286.706513	7999.868097	11.107776	-0.058769	4.815969
286.627684	7999.874155	11.112781	-0.058755	4.815971
286.575168	7999.855044	11.117786	-0.058745	4.815966
286.492122	8000.003153	11.122791	-0.058730	4.816010
286.661367	7999.858774	11.127795	-0.058761	4.815966
286.697130	8000.021871	11.132800	-0.058768	4.816014
286.522990	7999.863760	11.137805	-0.058736	4.815969
286.319390	7999.761751	11.142810	-0.058698	4.815940
286.469180	8000.026306	11.147815	-0.058726	4.816016
286.594636	7999.945248	11.152819	-0.058750	4.815992
286.339508	8000.156480	11.157824	-0.058702	4.816055
286.524868	8000.056209	11.162829	-0.058737	4.816025
286.687973	8000.146821	11.167834	-0.058768	4.816050
286.568618	7999.995048	11.172839	-0.058745	4.816007
286.512041	7999.848695	11.177843	-0.058735	4.815964
286.777919	7999.955069	11.182848	-0.058785	4.815994
286.574016	7999.962054	11.187853	-0.058747	4.815997
286.699345	7999.872445	11.192858	-0.058770	4.815970
286.497856	7999.983133	11.197863	-0.058733	4.816004
286.647611	7999.868321	11.202867	-0.058761	4.815969
286.516056	7999.841360	11.207872	-0.058736	4.815962
286.507457	7999.932049	11.212877	-0.058735	4.815989
286.665296	7999.820591	11.217882	-0.058764	4.815955
286.664526	7999.964855	11.222887	-0.058764	4.815997
286.790951	7999.861373	11.227891	-0.058788	4.815966
286.763932	7999.945316	11.232896	-0.058783	4.815991
286.456481	7999.776229	11.237901	-0.058726	4.815943
286.519218	7999.792344	11.242906	-0.058738	4.815948
286.710649	7999.858890	11.247911	-0.058774	4.815966
286.754196	7999.871450	11.252915	-0.058782	4.815970
286.664758	7999.862353	11.257920	-0.058765	4.815967
286.763722	7999.872716	11.262925	-0.058784	4.815970
286.593317	7999.867489	11.267930	-0.058752	4.815969
286.559884	8000.084895	11.272935	-0.058746	4.816033
286.649117	7999.858911	11.277939	-0.058763	4.815966
286.596410	8000.013985	11.282944	-0.058753	4.816012
286.526181	7999.995620	11.287949	-0.058740	4.816007
286.599540	7999.896515	11.292954	-0.058754	4.815978
286.667989	7999.950137	11.297959	-0.058767	4.815993
286.561365	7999.776157	11.302963	-0.058747	4.815943
286.429312	7999.951158	11.307968	-0.058723	4.815995
286.457986	7999.864064	11.312973	-0.058728	4.815969
286.640780	7999.875953	11.317978	-0.058762	4.815971
286.574278	7999.952765	11.322983	-0.058750	4.815994
286.806628	7999.788162	11.327987	-0.058793	4.815945
286.720427	7999.864615	11.332992	-0.058777	4.815968
286.707419	7999.904999	11.337997	-0.058775	4.815980
286.699519	7999.863190	11.343002	-0.058774	4.815967
286.535454	7999.970285	11.348007	-0.058743	4.816000
286.700486	7999.787358	11.353011	-0.058774	4.815945
286.602418	8000.028166	11.358016	-0.058756	4.816016
286.758610	7999.863245	11.363021	-0.058785	4.815967
286.817325	7999.883562	11.368026	-0.058796	4.815973
286.766265	8000.062177	11.373031	-0.058787	4.816025
286.629271	7999.874819	11.378035	-0.058762	4.815971
286.819901	7999.766094	11.383040	-0.058797	4.815938
286.579360	7999.888895	11.388045	-0.058753	4.815976
286.801284	7999.768985	11.393050	-0.058794	4.815939
286.813646	7999.978676	11.398055	-0.058796	4.816000
286.827070	7999.780165	11.403059	-0.058799	4.815942
286.717738	8000.013288	11.408064	-0.058779	4.816011
286.706937	7999.946847	11.413069	-0.058777	4.815992
286.810306	7999.881417	11.418074	-0.058796	4.815972
286.729060	7999.941931	11.423079	-0.058781	4.815990
286.830737	7999.783497	11.428083	-0.058800	4.815943
286.594309	7999.958737	11.433088	-0.058756	4.815996
286.412797	8000.028111	11.438093	-0.058723	4.816017
286.759192	7999.765133	11.443098	-0.058787	4.815938
286.532629	8000.011082	11.448103	-0.058745	4.816011
286.620878	7999.796835	11.453107	-0.058762	4.815948
286.555234	7999.853358	11.458112	-0.058750	4.815965
286.501812	7999.875908	11.463117	-0.058740	4.815972
286.784759	7999.851149	11.468122	-0.058793	4.815963
286.570134	7999.875038	11.473127	-0.058753	4.815971
286.662276	7999.881002	11.478131	-0.058770	4.815973
286.762800	7999.857197	11.483136	-0.058789	4.815965
286.587137	7999.917061	11.488141	-0.058756	4.815984
286.651664	7999.931071	11.493146	-0.058769	4.815987
286.646149	7999.949150	11.498151	-0.058768	4.815993
286.908243	7999.864168	11.503155	-0.058817	4.815966
286.564996	7999.981893	11.508160	-0.058753	4.816003
286.567092	7999.876147	11.513165	-0.058753	4.815972
286.670614	7999.781867	11.518170	-0.058773	4.815944
286.690615	7999.987422	11.523175	-0.058777	4.816004
286.781866	7999.873682	11.528179	-0.058794	4.815970
286.725480	7999.972051	11.533184	-0.058783	4.815999
286.698356	7999.996148	11.538189	-0.058778	4.816006
286.554611	7999.836452	11.543194	-0.058752	4.815960
286.568669	8000.033350	11.548199	-0.058755	4.816018
286.749845	7999.856060	11.553203	-0.058788	4.815965
286.992172	7999.976968	11.558208	-0.058834	4.815999
286.877173	8000.062515	11.563213	-0.058812	4.816025
286.956127	7999.966717	11.568218	-0.058827	4.815996
286.856782	7999.913625	11.573223	-0.058809	4.815981
286.817128	7999.849865	11.578227	-0.058801	4.815963
286.868197	7999.846532	11.583232	-0.058811	4.815961
286.850867	7999.991565	11.588237	-0.058808	4.816004
286.889032	7999.857622	11.593242	-0.058815	4.815965
286.860438	8000.009930	11.598247	-0.058810	4.816009
286.994924	7999.991018	11.603251	-0.058835	4.816003
287.017907	8000.048088	11.608256	-0.058840	4.816020
286.819464	7999.939757	11.613261	-0.058803	4.815989
286.960818	7999.904941	11.618266	-0.058829	4.815978
286.769422	7999.961312	11.623271	-0.058794	4.815995
286.997363	7999.806246	11.628275	-0.058836	4.815949
286.871987	8000.012362	11.633280	-0.058813	4.816010
286.886890	8000.005164	11.638285	-0.058816	4.816008
286.941607	7999.880072	11.643290	-0.058826	4.815971
286.891509	8000.045881	11.648295	-0.058817	4.816020
287.062338	7999.868402	11.653299	-0.058849	4.815967
287.146190	7999.854980	11.658304	-0.058865	4.815962
287.012352	7999.888889	11.663309	-0.058840	4.815973
287.033216	7999.885006	11.668314	-0.058844	4.815972
287.113974	8000.014727	11.673319	-0.058859	4.816009
287.132963	7999.940279	11.678323	-0.058863	4.815987
287.042331	8000.017721	11.683328	-0.058846	4.816010
286.840808	7999.883688	11.688333	-0.058809	4.815972
286.927287	7999.913059	11.693338	-0.058825	4.815981
286.677615	7999.860436	11.698343	-0.058778	4.815966
286.864248	7999.785835	11.703347	-0.058813	4.815944
287.025482	7999.984346	11.708352	-0.058844	4.816001
286.711463	7999.857882	11.713357	-0.058785	4.815966
286.730014	7999.773810	11.718362	-0.058789	4.815941
286.706697	8000.072618	11.723367	-0.058785	4.816028
286.782139	7999.969276	11.728371	-0.058799	4.815998
286.855984	7999.858424	11.733376	-0.058812	4.815965
286.841753	7999.971454	11.738381	-0.058810	4.815998
287.111025	7999.856680	11.743386	-0.058860	4.815963
286.805236	7999.781663	11.748391	-0.058803	4.815943
286.832133	7999.872999	11.753395	-0.058809	4.815969
286.741631	7999.853196	11.758400	-0.058792	4.815964
286.873375	7999.906902	11.763405	-0.058817	4.815979
286.925601	7999.887561	11.768410	-0.058826	4.815973
286.886808	8000.116627	11.773415	-0.058819	4.816040
286.975424	7999.857501	11.778419	-0.058836	4.815964
286.952158	7999.976778	11.783424	-0.058832	4.815999
286.805215	8000.109833	11.788429	-0.058805	4.816039
286.958813	7999.847617	11.793434	-0.058833	4.815961
286.704258	8000.104813	11.798439	-0.058786	4.816038
287.022124	7999.863754	11.803443	-0.058845	4.815966
286.965473	8000.030513	11.808448	-0.058835	4.816015
286.948352	8000.018458	11.813453	-0.058832	4.816011
287.017399	7999.901107	11.818458	-0.058845	4.815976
287.038013	7999.766845	11.823463	-0.058849	4.815937
286.912461	7999.903495	11.828467	-0.058825	4.815978
286.973006	7999.992239	11.833472	-0.058837	4.816003
287.099427	7999.874864	11.838477	-0.058860	4.815968
287.266626	7999.783879	11.843482	-0.058892	4.815941
287.040291	7999.859919	11.848487	-0.058850	4.815964
287.140348	7999.887400	11.853491	-0.058868	4.815972
287.049211	7999.869723	11.858496	-0.058852	4.815967
286.878716	7999.882660	11.863501	-0.058820	4.815972
287.065255	7999.879657	11.868506	-0.058855	4.815970
286.944115	7999.856090	11.873511	-0.058832	4.815964
287.047211	7999.891107	11.878515	-0.058852	4.815973
286.812572	7999.907151	11.883520	-0.058808	4.815979
286.958319	7999.792266	11.888525	-0.058835	4.815945
287.201136	7999.825553	11.893530	-0.058881	4.815953
286.983544	7999.836563	11.898535	-0.058840	4.815958
287.109281	7999.847414	11.903539	-0.058864	4.815960
286.810819	7999.894355	11.908544	-0.058808	4.815976
286.914641	7999.871679	11.913549	-0.058828	4.815968
286.944221	7999.847651	11.918554	-0.058833	4.815961
286.943241	7999.864743	11.923559	-0.058833	4.815966
286.908673	7999.859851	11.928563	-0.058827	4.815965
286.900722	7999.975132	11.933568	-0.058826	4.815999
286.956902	7999.776330	11.938573	-0.058836	4.815940
286.966121	7999.873757	11.943578	-0.058838	4.815969
286.854086	8000.122862	11.948583	-0.058818	4.816042
286.872925	7999.784455	11.953587	-0.058821	4.815943
286.981799	7999.875147	11.958592	-0.058841	4.815969
286.971722	8000.081226	11.963597	-0.058840	4.816029
286.943078	7999.925761	11.968602	-0.058835	4.815984
287.081674	7999.990279	11.973607	-0.058860	4.816002
287.135501	7999.872650	11.978611	-0.058871	4.815967
286.917927	7999.855877	11.983616	-0.058830	4.815964
287.136176	7999.857726	11.988621	-0.058871	4.815963
287.256056	7999.782978	11.993626	-0.058893	4.815941
287.131301	7999.946359	11.998631	-0.058870	4.815989
287.127027	7999.781721	12.003635	-0.058870	4.815941
287.077958	7999.885567	12.008640	-0.058861	4.815971
287.031504	7999.863360	12.013645	-0.058852	4.815965
287.184632	7999.862954	12.018650	-0.058881	4.815964
287.099879	7999.772725	12.023655	-0.058865	4.815938
287.174506	7999.879892	12.028659	-0.058879	4.815969
287.069039	7999.876915	12.033664	-0.058860	4.815969
286.877288	7999.892671	12.038669	-0.058824	4.815975
287.124285	7999.869396	12.043674	-0.058870	4.815966
286.844116	7999.869650	12.048679	-0.058818	4.815968
287.097034	7999.883885	12.053683	-0.058865	4.815971
287.065678	7999.867296	12.058688	-0.058860	4.815966
287.238389	7999.862973	12.063693	-0.058892	4.815964
287.115089	7999.857533	12.068698	-0.058869	4.815963
287.048670	7999.985643	12.073703	-0.058857	4.816001
287.134828	7999.972263	12.078707	-0.058873	4.815996
287.143118	7999.968151	12.083712	-0.058875	4.815995
287.000904	8000.029693	12.088717	-0.058848	4.816014
287.133913	7999.976557	12.093722	-0.058873	4.815998
286.987388	7999.862760	12.098727	-0.058846	4.815965
286.776651	7999.801228	12.103731	-0.058807	4.815948
286.909469	7999.959681	12.108736	-0.058832	4.815994
286.780698	7999.893229	12.113741	-0.058808	4.815975
286.914489	7999.886060	12.118746	-0.058833	4.815972
286.902319	8000.031187	12.123751	-0.058831	4.816015
286.996220	7999.961309	12.128755	-0.058848	4.815994
286.882163	7999.822457	12.133760	-0.058827	4.815954
286.883908	7999.996691	12.138765	-0.058828	4.816005
287.025273	7999.868901	12.143770	-0.058854	4.815967
287.128377	8000.013991	12.148775	-0.058873	4.816009
287.194221	7999.883757	12.153779	-0.058886	4.815970
287.350058	7999.865234	12.158784	-0.058915	4.815964
287.052490	7999.918603	12.163789	-0.058860	4.815981
287.025347	7999.888198	12.168794	-0.058855	4.815972
286.987700	7999.999733	12.173799	-0.058848	4.816005
287.037268	7999.923705	12.178803	-0.058857	4.815983
287.093056	7999.941831	12.183808	-0.058868	4.815988
287.141760	7999.895709	12.188813	-0.058877	4.815974
287.236574	7999.796995	12.193818	-0.058895	4.815945
287.131088	7999.859205	12.198823	-0.058875	4.815963
287.226587	7999.879123	12.203827	-0.058893	4.815969
287.058480	7999.868593	12.208832	-0.058862	4.815966
287.124503	7999.874082	12.213837	-0.058874	4.815968
287.270546	7999.772025	12.218842	-0.058902	4.815937
287.059290	7999.993677	12.223847	-0.058862	4.816003
287.286864	7999.876006	12.228851	-0.058905	4.815967
287.388774	7999.860775	12.233856	-0.058924	4.815962
287.202149	7999.774034	12.238861	-0.058889	4.815938
287.294635	7999.808858	12.243866	-0.058907	4.815948
287.280508	7999.869526	12.248871	-0.058904	4.815966
287.237894	7999.902959	12.253875	-0.058896	4.815976
287.259563	7999.848864	12.258880	-0.058901	4.815960
287.315531	7999.972792	12.263885	-0.058911	4.815995
287.221212	7999.786208	12.268890	-0.058894	4.815941
287.131587	7999.860462	12.273895	-0.058877	4.815964
287.163184	7999.791587	12.278899	-0.058883	4.815943
287.041599	7999.865260	12.283904	-0.058861	4.815966
287.022158	7999.864917	12.288909	-0.058857	4.815966
286.999502	7999.787574	12.293914	-0.058853	4.815943
287.092770	7999.868365	12.298919	-0.058870	4.815966
287.159771	7999.901656	12.303923	-0.058883	4.815976
287.063397	7999.778087	12.308928	-0.058865	4.815940
287.056220	7999.889108	12.313933	-0.058864	4.815972
287.295280	7999.798363	12.318938	-0.058909	4.815945
287.112218	7999.876259	12.323943	-0.058875	4.815968
287.139153	7999.792338	12.328947	-0.058880	4.815944
287.198526	7999.901365	12.333952	-0.058891	4.815975
287.190196	7999.877715	12.338957	-0.058890	4.815968
287.271268	7999.812947	12.343962	-0.058905	4.815949
287.341086	7999.774690	12.348967	-0.058918	4.815937
287.129235	7999.994193	12.353971	-0.058879	4.816003
287.147356	7999.965682	12.358976	-0.058882	4.815994
286.944007	7999.829477	12.363981	-0.058844	4.815956
287.132968	7999.868196	12.368986	-0.058880	4.815966
286.851530	7999.946438	12.373991	-0.058827	4.815990
286.981896	7999.802418	12.378995	-0.058852	4.815947
287.070288	7999.794422	12.384000	-0.058868	4.815945
287.103772	7999.972440	12.389005	-0.058875	4.815996
287.273927	7999.852656	12.394010	-0.058906	4.815961
287.306194	7999.779518	12.399015	-0.058913	4.815939
287.279497	7999.906214	12.404019	-0.058908	4.815976
287.174834	7999.867985	12.409024	-0.058888	4.815966
287.391938	7999.867677	12.414029	-0.058929	4.815964
287.436413	7999.884528	12.419034	-0.058937	4.815969
287.256996	7999.871655	12.424039	-0.058904	4.815966
287.256323	7999.786162	12.429043	-0.058904	4.815941
287.225288	7999.864689	12.434048	-0.058898	4.815964
287.095473	7999.864475	12.439053	-0.058874	4.815965
287.222846	7999.872150	12.444058	-0.058898	4.815966
287.257265	7999.887750	12.449063	-0.058905	4.815971
287.321896	7999.782073	12.454067	-0.058917	4.815940
287.214573	7999.785474	12.459072	-0.058897	4.815941
287.307579	7999.985950	12.464077	-0.058915	4.815999
287.423331	7999.795711	12.469082	-0.058936	4.815943
287.204344	8000.123021	12.474087	-0.058896	4.816040
287.400530	7999.773947	12.479091	-0.058932	4.815937
287.416440	7999.883252	12.484096	-0.058935	4.815969
287.207949	8000.003431	12.489101	-0.058897	4.816005
287.307096	7999.886628	12.494106	-0.058915	4.815970
287.313212	7999.972244	12.499111	-0.058916	4.815995
287.423280	7999.871669	12.504115	-0.058937	4.815965
287.277735	7999.799568	12.509120	-0.058910	4.815945
287.393342	7999.845500	12.514125	-0.058932	4.815958
287.464889	7999.867120	12.519130	-0.058945	4.815964
287.233861	7999.869336	12.524135	-0.058902	4.815966
287.327788	7999.799458	12.529139	-0.058920	4.815945
287.324982	7999.874225	12.534144	-0.058919	4.815966
287.367788	7999.784181	12.539149	-0.058927	4.815940
287.425283	7999.905999	12.544154	-0.058938	4.815975
287.258212	7999.771523	12.549159	-0.058907	4.815937
287.293934	7999.879051	12.554163	-0.058914	4.815968
287.252240	7999.769301	12.559168	-0.058906	4.815936
287.375234	7999.890174	12.564173	-0.058930	4.815971
287.425222	7999.829114	12.569178	-0.058939	4.815953
287.230952	7999.830931	12.574183	-0.058903	4.815954
287.252434	7999.897591	12.579187	-0.058907	4.815974
287.386542	7999.784630	12.584192	-0.058932	4.815940
287.345167	7999.928158	12.589197	-0.058925	4.815982
287.409364	7999.864151	12.594202	-0.058937	4.815963
287.131942	7999.865522	12.599207	-0.058885	4.815965
287.410365	7999.786181	12.604211	-0.058937	4.815940
287.292510	7999.796870	12.609216	-0.058915	4.815944
287.161404	7999.888537	12.614221	-0.058891	4.815971
287.286355	7999.802126	12.619226	-0.058914	4.815946
287.175828	7999.874931	12.624231	-0.058894	4.815967
287.198949	7999.802695	12.629235	-0.058898	4.815946
287.529649	7999.802318	12.634240	-0.058960	4.815944
287.477743	7999.908251	12.639245	-0.058950	4.815976
287.634059	7999.812792	12.644250	-0.058980	4.815947
287.637678	7999.780810	12.649255	-0.058980	4.815937
287.523592	7999.792637	12.654259	-0.058959	4.815941
287.514454	7999.797826	12.659264	-0.058958	4.815943
287.438226	7999.884080	12.664269	-0.058944	4.815969
287.434649	7999.797465	12.669274	-0.058943	4.815943
287.278196	7999.795697	12.674279	-0.058914	4.815944
287.517503	7999.896247	12.679283	-0.058959	4.815972
287.335377	7999.901491	12.684288	-0.058925	4.815974
287.355800	7999.978819	12.689293	-0.058929	4.815997
287.283340	7999.864233	12.694298	-0.058916	4.815964
287.282952	7999.877061	12.699303	-0.058916	4.815967
287.500365	7999.795540	12.704307	-0.058956	4.815942
287.425309	7999.794185	12.709312	-0.058942	4.815942
287.475136	7999.966091	12.714317	-0.058952	4.815992
287.654748	7999.794113	12.719322	-0.058985	4.815941
287.445078	7999.884349	12.724327	-0.058946	4.815969
287.416045	7999.780172	12.729331	-0.058941	4.815938
287.497735	7999.898156	12.734336	-0.058957	4.815972
287.473140	7999.805815	12.739341	-0.058952	4.815946
287.407791	7999.800362	12.744346	-0.058940	4.815944
287.346450	7999.780021	12.749351	-0.058929	4.815939
287.340538	7999.903890	12.754355	-0.058928	4.815975
287.292408	7999.866691	12.759360	-0.058919	4.815964
287.237927	7999.877466	12.764365	-0.058909	4.815968
287.477159	7999.789930	12.769370	-0.058953	4.815941
287.336300	7999.876075	12.774375	-0.058927	4.815967
287.277818	7999.787393	12.779379	-0.058917	4.815941
287.429326	7999.800850	12.784384	-0.058945	4.815944
287.361136	7999.888319	12.789389	-0.058932	4.815970
287.520098	7999.792909	12.794394	-0.058962	4.815941
287.321461	7999.882277	12.799399	-0.058925	4.815969
287.316293	7999.883264	12.804403	-0.058924	4.815969
287.299116	7999.782509	12.809408	-0.058921	4.815940
287.379395	7999.981685	12.814413	-0.058937	4.815997
287.558591	7999.793670	12.819418	-0.058970	4.815941
287.623283	7999.775624	12.824423	-0.058982	4.815936
287.528833	7999.880783	12.829427	-0.058965	4.815967
287.339252	7999.777957	12.834432	-0.058929	4.815938
287.609850	7999.883351	12.839437	-0.058980	4.815967
287.625332	7999.890057	12.844442	-0.058983	4.815969
287.635905	7999.869957	12.849447	-0.058985	4.815963
287.493392	7999.882334	12.854451	-0.058959	4.815968
287.473401	7999.814656	12.859456	-0.058955	4.815948
287.361781	7999.780576	12.864461	-0.058934	4.815939
287.730309	7999.803330	12.869466	-0.059003	4.815943
287.530766	7999.859552	12.874471	-0.058966	4.815961
287.361936	7999.890687	12.879475	-0.058935	4.815971
287.387636	7999.867656	12.884480	-0.058940	4.815964
287.514769	7999.786628	12.889485	-0.058963	4.815940
287.595223	7999.800929	12.894490	-0.058979	4.815943
287.465887	7999.873392	12.899495	-0.058955	4.815965
287.402941	7999.772872	12.904499	-0.058943	4.815936
287.679208	7999.875164	12.909504	-0.058995	4.815965
287.504798	7999.793987	12.914509	-0.058962	4.815942
287.662667	7999.816110	12.919514	-0.058992	4.815947
287.494863	7999.786349	12.924519	-0.058961	4.815940
287.403984	7999.904396	12.929523	-0.058944	4.815975
287.279771	7999.882910	12.934528	-0.058921	4.815969
287.316133	7999.904958	12.939533	-0.058928	4.815975
287.350717	7999.858578	12.944538	-0.058934	4.815961
287.323619	7999.979924	12.949543	-0.058929	4.815997
287.282139	7999.809264	12.954547	-0.058922	4.815947
287.507502	7999.881774	12.959552	-0.058964	4.815967
287.321723	7999.905119	12.964557	-0.058929	4.815975
287.533262	7999.810667	12.969562	-0.058969	4.815946
287.621878	7999.895649	12.974567	-0.058986	4.815971
287.470353	7999.810614	12.979571	-0.058957	4.815947
287.326703	7999.781293	12.984576	-0.058931	4.815939
287.450071	7999.892556	12.989581	-0.058954	4.815971
287.449836	7999.809208	12.994586	-0.058954	4.815946
287.345259	7999.776324	12.999591	-0.058935	4.815937
287.320508	7999.893438	13.004595	-0.058930	4.815972
287.450956	7999.785753	13.009600	-0.058954	4.815940
287.540946	7999.882515	13.014605	-0.058971	4.815967
287.645891	7999.831006	13.019610	-0.058991	4.815952
287.356530	7999.815061	13.024615	-0.058937	4.815949
287.633587	7999.796608	13.029619	-0.058989	4.815942
287.613599	7999.810149	13.034624	-0.058985	4.815946
287.317443	7999.946899	13.039629	-0.058930	4.815987
287.611441	7999.818683	13.044634	-0.058985	4.815948
287.518466	7999.779598	13.049639	-0.058968	4.815937
287.418537	7999.795958	13.054643	-0.058950	4.815943
287.744391	7999.877780	13.059648	-0.059010	4.815965
287.345121	7999.998759	13.064653	-0.058936	4.816002
287.522570	7999.778652	13.069658	-0.058969	4.815937
287.473141	7999.865394	13.074663	-0.058960	4.815963
287.553094	7999.873275	13.079667	-0.058975	4.815965
287.561874	7999.901232	13.084672	-0.058977	4.815973
287.717273	7999.798276	13.089677	-0.059006	4.815942
287.765756	7999.807721	13.094682	-0.059015	4.815944
287.360839	7999.783259	13.099687	-0.058940	4.815939
287.413233	7999.813079	13.104691	-0.058950	4.815948
287.531481	7999.807764	13.109696	-0.058972	4.815946
287.586907	7999.869700	13.114701	-0.058982	4.815963
287.774812	7999.805808	13.119706	-0.059017	4.815944
287.546475	7999.870056	13.124711	-0.058975	4.815964
287.525167	7999.804491	13.129715	-0.058971	4.815945
287.439725	7999.791192	13.134720	-0.058955	4.815941
287.629090	7999.894039	13.139725	-0.058991	4.815970
287.796970	7999.825508	13.144730	-0.059022	4.815949
287.821947	7999.814219	13.149735	-0.059027	4.815946
287.410986	7999.877278	13.154739	-0.058951	4.815966
287.589243	7999.867713	13.159744	-0.058984	4.815963
287.467647	7999.854823	13.164749	-0.058961	4.815960
287.784133	7999.836020	13.169754	-0.059020	4.815952
287.626811	7999.910111	13.174759	-0.058991	4.815975
287.602434	7999.823117	13.179763	-0.058987	4.815950
287.625061	7999.817129	13.184768	-0.058991	4.815948
287.390403	7999.868438	13.189773	-0.058948	4.815964
287.750192	7999.805539	13.194778	-0.059015	4.815944
287.424860	7999.857334	13.199783	-0.058954	4.815961
287.482602	7999.788934	13.204787	-0.058965	4.815940
287.595334	7999.825197	13.209792	-0.058986	4.815950
287.633519	7999.970175	13.214797	-0.058994	4.815992
287.539424	7999.824203	13.219802	-0.058976	4.815950
287.511956	7999.796998	13.224807	-0.058971	4.815942
287.561573	7999.811806	13.229811	-0.058980	4.815946
287.518270	7999.780038	13.234816	-0.058973	4.815937
287.401587	7999.867693	13.239821	-0.058951	4.815964
287.582311	7999.872065	13.244826	-0.058985	4.815964
287.506596	7999.864286	13.249831	-0.058971	4.815962
287.395919	7999.822741	13.254835	-0.058950	4.815951
287.401642	7999.788661	13.259840	-0.058951	4.815941
287.400973	7999.866673	13.264845	-0.058951	4.815963
287.218427	7999.797103	13.269850	-0.058918	4.815944
287.360728	7999.768716	13.274855	-0.058944	4.815935
287.356489	7999.878722	13.279859	-0.058944	4.815967
287.442766	7999.786263	13.284864	-0.058960	4.815940
287.335675	7999.865543	13.289869	-0.058940	4.815963
287.537981	7999.819013	13.294874	-0.058978	4.815949
287.365623	7999.922752	13.299879	-0.058946	4.815980
287.447278	7999.900741	13.304883	-0.058961	4.815973
287.558401	7999.790567	13.309888	-0.058982	4.815940
287.684254	8000.007674	13.314893	-0.059006	4.816003
287.538272	7999.873580	13.319898	-0.058978	4.815965
287.387028	8000.000146	13.324903	-0.058950	4.816002
287.668066	7999.884517	13.329907	-0.059003	4.815967
287.597706	7999.776381	13.334912	-0.058990	4.815936
287.600518	7999.975217	13.339917	-0.058991	4.815994
287.610117	7999.873880	13.344922	-0.058992	4.815964
287.530173	7999.861749	13.349927	-0.058978	4.815961
287.614976	7999.838726	13.354931	-0.058994	4.815954
287.743643	7999.843219	13.359936	-0.059018	4.815955
287.679159	7999.785417	13.364941	-0.059006	4.815938
287.660541	7999.879133	13.369946	-0.059002	4.815966
287.442698	7999.864490	13.374951	-0.058962	4.815962
287.747859	7999.810215	13.379955	-0.059019	4.815945
287.860038	7999.802652	13.384960	-0.059040	4.815942
287.605096	7999.788403	13.389965	-0.058992	4.815939
287.820767	7999.890661	13.394970	-0.059033	4.815968
287.676947	7999.774774	13.399975	-0.059006	4.815935
287.542948	7999.877075	13.404979	-0.058981	4.815966
287.480152	7999.883424	13.409984	-0.058970	4.815968
287.455348	7999.970615	13.414989	-0.058965	4.815993
287.516443	7999.805027	13.419994	-0.058977	4.815945
287.439474	7999.870963	13.424999	-0.058963	4.815964
287.528618	7999.939925	13.430003	-0.058979	4.815984
287.538603	7999.915540	13.435008	-0.058981	4.815977
287.386024	7999.989717	13.440013	-0.058953	4.815999
287.354023	7999.782894	13.445018	-0.058947	4.815939
287.390055	7999.861574	13.450023	-0.058954	4.815962
287.457228	7999.883114	13.455027	-0.058967	4.815968
287.438097	7999.868885	13.460032	-0.058963	4.815964
287.477359	7999.893123	13.465037	-0.058971	4.815971
287.606928	7999.812139	13.470042	-0.058995	4.815946
287.544656	7999.870862	13.475047	-0.058983	4.815964
287.610941	7999.809030	13.480051	-0.058996	4.815945
287.954215	7999.793921	13.485056	-0.059060	4.815939
287.495307	7999.970454	13.490061	-0.058975	4.815993
287.603308	7999.861291	13.495066	-0.058995	4.815961
287.645864	7999.857804	13.500071	-0.059003	4.815959
287.473962	7999.988268	13.505075	-0.058971	4.815998
287.678753	7999.875526	13.510080	-0.059009	4.815964
287.715803	8000.015141	13.515085	-0.059016	4.816005
287.688836	7999.852222	13.520090	-0.059011	4.815957
287.698720	7999.849208	13.525095	-0.059013	4.815956
287.768658	7999.903928	13.530099	-0.059026	4.815972
287.778539	7999.872060	13.535104	-0.059028	4.815963
287.587824	7999.891040	13.540109	-0.058993	4.815969
287.629530	7999.860820	13.545114	-0.059001	4.815960
287.739335	7999.887412	13.550119	-0.059021	4.815967
287.678474	7999.872422	13.555123	-0.059010	4.815963
287.634655	7999.898353	13.560128	-0.059002	4.815971
287.685424	7999.868298	13.565133	-0.059012	4.815962
287.649681	7999.794990	13.570138	-0.059005	4.815941
287.585092	7999.901761	13.575143	-0.058993	4.815972
287.705452	7999.981979	13.580147	-0.059016	4.815995
287.955783	7999.792052	13.585152	-0.059063	4.815938
287.517537	7999.971099	13.590157	-0.058981	4.815993
287.531762	7999.798245	13.595162	-0.058984	4.815942
287.667461	7999.889428	13.600167	-0.059009	4.815968
287.708355	7999.799348	13.605171	-0.059017	4.815942
287.689898	7999.891998	13.610176	-0.059014	4.815969
287.834362	7999.784569	13.615181	-0.059041	4.815937
287.926765	7999.820461	13.620186	-0.059058	4.815947
287.821572	7999.874128	13.625191	-0.059039	4.815963
287.825835	7999.807960	13.630195	-0.059039	4.815944
287.806203	7999.809752	13.635200	-0.059036	4.815944
287.626846	7999.906952	13.640205	-0.059003	4.815974
287.812068	7999.868660	13.645210	-0.059037	4.815961
287.839066	7999.871301	13.650215	-0.059042	4.815962
287.749269	7999.897463	13.655219	-0.059026	4.815970
287.710094	7999.876456	13.660224	-0.059019	4.815964
287.703220	7999.863519	13.665229	-0.059018	4.815961
287.929069	7999.797112	13.670234	-0.059060	4.815940
287.768166	7999.883962	13.675239	-0.059030	4.815966
287.835631	7999.979247	13.680243	-0.059043	4.815994
288.020389	7999.871482	13.685248	-0.059077	4.815961
287.866237	7999.893265	13.690253	-0.059049	4.815968
287.737724	7999.827884	13.695258	-0.059025	4.815950
287.897824	7999.953711	13.700263	-0.059055	4.815986
287.875748	7999.785538	13.705267	-0.059051	4.815937
288.003727	7999.799637	13.710272	-0.059075	4.815940
288.001804	7999.884039	13.715277	-0.059074	4.815965
288.126276	7999.784794	13.720282	-0.059098	4.815935
287.845018	7999.886551	13.725287	-0.059045	4.815966
287.632066	7999.859173	13.730291	-0.059006	4.815960
287.807213	7999.810010	13.735296	-0.059039	4.815944
287.872395	7999.861437	13.740301	-0.059051	4.815959
287.751240	7999.804740	13.745306	-0.059028	4.815943
287.598409	7999.875706	13.750311	-0.059000	4.815965
287.702242	7999.782498	13.755315	-0.059020	4.815937
287.691611	7999.892389	13.760320	-0.059018	4.815969
287.793325	7999.775631	13.765325	-0.059037	4.815934
287.854076	7999.902854	13.770330	-0.059048	4.815971
287.675845	7999.783134	13.775335	-0.059015	4.815937
287.663904	7999.893001	13.780339	-0.059013	4.815969
287.842016	7999.790459	13.785344	-0.059046	4.815938
288.081271	7999.868568	13.790349	-0.059091	4.815960
287.876518	7999.803935	13.795354	-0.059053	4.815942
287.822097	7999.879901	13.800359	-0.059043	4.815965
287.948631	7999.910004	13.805363	-0.059067	4.815973
287.859129	7999.791899	13.810368	-0.059050	4.815939
287.630478	7999.878583	13.815373	-0.059008	4.815965
287.984870	7999.942760	13.820378	-0.059074	4.815982
287.865781	8000.021823	13.825383	-0.059052	4.816006
287.784965	7999.787390	13.830387	-0.059037	4.815938
287.908494	7999.815301	13.835392	-0.059060	4.815945
287.716810	7999.879147	13.840397	-0.059024	4.815965
287.844201	7999.814153	13.845402	-0.059048	4.815945
287.708155	7999.880082	13.850407	-0.059023	4.815965
287.798635	7999.777013	13.855411	-0.059040	4.815935
287.641744	7999.870347	13.860416	-0.059011	4.815963
287.616685	7999.962877	13.865421	-0.059006	4.815990
287.843358	7999.788550	13.870426	-0.059049	4.815938
287.824115	7999.873705	13.875431	-0.059045	4.815963
287.836829	7999.870743	13.880435	-0.059048	4.815962
287.853621	7999.884954	13.885440	-0.059051	4.815966
287.736096	7999.868932	13.890445	-0.059029	4.815962
288.015866	7999.868697	13.895450	-0.059081	4.815960
287.778315	7999.878274	13.900455	-0.059037	4.815964
287.775079	7999.986164	13.905459	-0.059037	4.815996
287.960866	7999.793992	13.910464	-0.059071	4.815939
287.818802	7999.872636	13.915469	-0.059045	4.815962
287.604353	7999.883703	13.920474	-0.059005	4.815967
287.849648	7999.785590	13.925479	-0.059051	4.815937
287.605334	7999.870920	13.930483	-0.059006	4.815963
287.848841	7999.902085	13.935488	-0.059051	4.815971
287.944459	7999.872847	13.940493	-0.059069	4.815962
288.051521	7999.814964	13.945498	-0.059089	4.815944
287.931886	7999.810659	13.950503	-0.059067	4.815944
288.099605	7999.900290	13.955507	-0.059098	4.815969
287.908283	7999.785674	13.960512	-0.059063	4.815936
287.748953	7999.954840	13.965517	-0.059033	4.815987
287.795366	7999.919362	13.970522	-0.059042	4.815976
287.766026	7999.880368	13.975527	-0.059037	4.815965
287.794985	7999.899075	13.980531	-0.059042	4.815970
287.745508	7999.812691	13.985536	-0.059033	4.815945
287.708852	8000.104854	13.990541	-0.059027	4.816031
287.741269	7999.869278	13.995546	-0.059033	4.815962
287.700343	7999.862132	14.000551	-0.059025	4.815960
287.580827	7999.883478	14.005555	-0.059003	4.815967
287.765701	7999.892201	14.010560	-0.059038	4.815968
287.638393	7999.781958	14.015565	-0.059014	4.815937
287.767472	7999.818519	14.020570	-0.059038	4.815947
287.845382	7999.826362	14.025575	-0.059053	4.815949
287.759289	7999.961596	14.030579	-0.059037	4.815989
287.993341	7999.797021	14.035584	-0.059081	4.815939
288.080817	7999.871297	14.040589	-0.059097	4.815961
288.259198	7999.818987	14.045594	-0.059130	4.815944
287.987135	7999.831141	14.050599	-0.059080	4.815949
287.911423	7999.792371	14.055603	-0.059066	4.815938
287.982630	7999.903754	14.060608	-0.059079	4.815971
287.941150	7999.785455	14.065613	-0.059072	4.815936
287.822094	7999.899784	14.070618	-0.059050	4.815970
287.874103	7999.777846	14.075623	-0.059059	4.815934
287.788762	7999.937673	14.080627	-0.059044	4.815981
287.839528	7999.886245	14.085632	-0.059053	4.815966
287.617703	7999.886491	14.090637	-0.059012	4.815967
287.754113	7999.812043	14.095642	-0.059038	4.815945
287.638141	7999.801393	14.100647	-0.059016	4.815942
287.706103	7999.874244	14.105651	-0.059029	4.815963
287.929281	7999.830231	14.110656	-0.059071	4.815949
287.752098	7999.867625	14.115661	-0.059038	4.815961
287.807449	7999.816281	14.120666	-0.059048	4.815946
288.115346	7999.788772	14.125671	-0.059106	4.815936
288.105893	7999.883725	14.130675	-0.059104	4.815964
287.922139	7999.882526	14.135680	-0.059070	4.815965
287.756049	7999.894474	14.140685	-0.059039	4.815969
287.868086	7999.875154	14.145690	-0.059060	4.815963
287.746627	7999.890052	14.150695	-0.059038	4.815968
287.766148	7999.918205	14.155699	-0.059041	4.815976
287.942654	7999.795329	14.160704	-0.059074	4.815939
287.852254	7999.881325	14.165709	-0.059058	4.815965
287.755510	7999.796218	14.170714	-0.059040	4.815940
287.888099	7999.787959	14.175719	-0.059064	4.815937
287.801037	7999.870810	14.180723	-0.059048	4.815962
287.830262	7999.783723	14.185728	-0.059054	4.815936
287.910477	7999.866416	14.190733	-0.059069	4.815960
288.038373	7999.881582	14.195738	-0.059093	4.815964
288.062677	7999.875625	14.200743	-0.059098	4.815962
287.982916	7999.870977	14.205747	-0.059083	4.815961
288.129667	7999.798855	14.210752	-0.059110	4.815939
287.905158	7999.884546	14.215757	-0.059069	4.815965
287.798766	7999.786439	14.220762	-0.059049	4.815937
287.754083	7999.902123	14.225767	-0.059041	4.815971
287.992223	7999.872276	14.230771	-0.059085	4.815961
287.931099	7999.894685	14.235776	-0.059074	4.815968
287.983010	7999.778088	14.240781	-0.059084	4.815934
288.078400	7999.888843	14.245786	-0.059102	4.815966
288.005903	7999.777460	14.250791	-0.059088	4.815933
287.686945	7999.902041	14.255795	-0.059029	4.815971
287.803175	7999.567539	14.260800	-0.059051	4.815873

287.728736	7996.313530	14.265805	-0.059035	4.814923
287.733215	7990.743699	14.270810	-0.059032	4.813295
287.869649	7983.963087	14.275815	-0.059053	4.811312
287.802649	7976.629906	14.280819	-0.059036	4.809167
287.705033	7969.054156	14.285824	-0.059013	4.806951
287.976384	7961.234569	14.290829	-0.059059	4.804660
287.789708	7953.377758	14.295834	-0.059019	4.802360
287.689677	7945.429327	14.300839	-0.058995	4.800031
287.490756	7937.425659	14.305843	-0.058953	4.797686
287.618489	7929.433507	14.310848	-0.058972	4.795341
287.442398	7921.374331	14.315853	-0.058934	4.792977
287.308087	7913.392167	14.320858	-0.058904	4.790634
287.403245	7905.395306	14.325863	-0.058916	4.788284
287.333914	7897.395509	14.330867	-0.058898	4.785933
287.265578	7889.441091	14.335872	-0.058881	4.783594
287.221865	7881.412465	14.340877	-0.058867	4.781233
287.305101	7873.423685	14.345882	-0.058878	4.778881
287.082911	7865.421535	14.350887	-0.058831	4.776525
286.901892	7857.408142	14.355891	-0.058792	4.774165
287.051237	7849.394065	14.360896	-0.058815	4.771802
286.993948	7841.382002	14.365901	-0.058799	4.769439
287.013556	7833.368682	14.370906	-0.058798	4.767075
287.079897	7825.386423	14.375911	-0.058805	4.764718
287.037047	7817.403423	14.380915	-0.058792	4.762360
286.920861	7809.354753	14.385920	-0.058765	4.759982
286.731678	7801.428474	14.390925	-0.058725	4.757639
286.805212	7793.359811	14.395930	-0.058734	4.755252
286.700520	7785.358252	14.400935	-0.058709	4.752885
286.466427	7777.238910	14.405939	-0.058660	4.750481
286.752459	7769.378960	14.410944	-0.058709	4.748152
286.719707	7761.332428	14.415949	-0.058697	4.745767
286.563906	7753.382135	14.420954	-0.058663	4.743410
286.460443	7745.358643	14.425959	-0.058639	4.741029
286.470699	7737.322697	14.430963	-0.058636	4.738644
286.582360	7729.341373	14.435968	-0.058651	4.736273
286.444783	7721.319150	14.440973	-0.058621	4.733890
286.221222	7713.349407	14.445978	-0.058574	4.731521
286.281101	7705.312372	14.450983	-0.058580	4.729130
286.153758	7697.307775	14.455987	-0.058551	4.726748
286.241442	7689.290687	14.460992	-0.058562	4.724361
286.167569	7681.338804	14.465997	-0.058544	4.721992
286.173188	7673.310080	14.471002	-0.058540	4.719599
286.031119	7665.395944	14.476007	-0.058508	4.717240
286.095173	7657.303742	14.481011	-0.058515	4.714825
286.117063	7649.282180	14.486016	-0.058514	4.712431
286.013534	7641.255148	14.491021	-0.058489	4.710033
285.897860	7633.352260	14.496026	-0.058463	4.707672
285.944980	7625.300353	14.501031	-0.058467	4.705265
285.705280	7617.315751	14.506035	-0.058417	4.702877
285.653839	7609.317123	14.511040	-0.058402	4.700484
285.618540	7601.324819	14.516045	-0.058390	4.698091
285.491613	7593.328557	14.521050	-0.058362	4.695695
285.782478	7585.300242	14.526055	-0.058411	4.693288
285.636095	7577.233980	14.531059	-0.058378	4.690870
285.699245	7569.362884	14.536064	-0.058385	4.688508
285.470722	7561.276245	14.541069	-0.058337	4.686081
285.433205	7553.318952	14.546074	-0.058325	4.683691
285.534153	7545.322066	14.551079	-0.058339	4.681288
285.449355	7537.272951	14.556083	-0.058318	4.678868
285.348248	7529.309900	14.561088	-0.058294	4.676473
285.313987	7521.178227	14.566093	-0.058283	4.674025
285.170682	7513.175561	14.571098	-0.058251	4.671616
284.964083	7505.232641	14.576103	-0.058207	4.669223
284.961679	7497.213295	14.581107	-0.058202	4.666806
284.978246	7489.260315	14.586112	-0.058200	4.664407
284.919794	7481.281016	14.591117	-0.058184	4.661999
285.043571	7473.236546	14.596122	-0.058202	4.659570
284.890038	7465.304328	14.601127	-0.058168	4.657175
284.870821	7457.215819	14.606131	-0.058160	4.654730
285.056818	7449.238869	14.611136	-0.058189	4.652318
284.830841	7441.196019	14.616141	-0.058142	4.649885
284.784948	7433.243846	14.621146	-0.058128	4.647478
284.708167	7425.224580	14.626151	-0.058109	4.645049
284.702203	7417.241760	14.631155	-0.058103	4.642630
284.789394	7409.223313	14.636160	-0.058114	4.640199
284.587707	7401.261510	14.641165	-0.058071	4.637784
284.604708	7393.206985	14.646170	-0.058069	4.635340
284.424892	7385.216725	14.651175	-0.058031	4.632913
284.240958	7377.168049	14.656179	-0.057991	4.630468
284.529193	7369.240031	14.661184	-0.058040	4.628058
284.364329	7361.191705	14.666189	-0.058004	4.625610
284.326689	7353.232126	14.671194	-0.057992	4.623188
284.181263	7345.206791	14.676199	-0.057960	4.620745
284.263017	7337.214916	14.681203	-0.057970	4.618311
284.441006	7329.190542	14.686208	-0.057998	4.615865
284.349469	7321.150470	14.691213	-0.057976	4.613413
284.261244	7313.159733	14.696218	-0.057954	4.610975
284.245279	7305.234701	14.701223	-0.057946	4.608556
283.991539	7297.144981	14.706227	-0.057894	4.606085
283.936300	7289.183463	14.711232	-0.057879	4.603652
283.787422	7281.208767	14.716237	-0.057846	4.601214
283.656995	7273.172057	14.721242	-0.057816	4.598755
283.558320	7265.202934	14.726247	-0.057793	4.596316
283.645734	7257.128033	14.731251	-0.057804	4.593843
283.675328	7249.091076	14.736256	-0.057805	4.591380
283.628262	7241.062523	14.741261	-0.057791	4.588919
283.561254	7233.117682	14.746266	-0.057773	4.586482
283.547742	7225.128245	14.751271	-0.057766	4.584030
283.578193	7217.175582	14.756275	-0.057766	4.581588
283.532539	7209.215049	14.761280	-0.057753	4.579142
283.478686	7201.164378	14.766285	-0.057737	4.576667
283.500301	7193.146394	14.771290	-0.057736	4.574201
283.189210	7185.094753	14.776295	-0.057673	4.571723
283.181802	7177.090625	14.781299	-0.057667	4.569259
283.316925	7169.172594	14.786304	-0.057687	4.566820
283.177648	7161.104446	14.791309	-0.057656	4.564333
283.157678	7153.171016	14.796314	-0.057647	4.561886
283.194332	7145.152697	14.801319	-0.057649	4.559412
282.888797	7137.130603	14.806323	-0.057587	4.556935
282.820338	7129.121369	14.811328	-0.057569	4.554461
282.944337	7121.080553	14.816333	-0.057587	4.551976
282.719312	7113.125023	14.821338	-0.057540	4.549515
282.727471	7105.126643	14.826343	-0.057536	4.547040
282.632436	7097.075552	14.831347	-0.057514	4.544548
282.859076	7089.170710	14.836352	-0.057551	4.542099
282.800965	7081.109112	14.841357	-0.057535	4.539601
282.711968	7073.151766	14.846362	-0.057513	4.537133
282.778305	7065.118604	14.851367	-0.057520	4.534641
282.813826	7057.086972	14.856371	-0.057522	4.532148
282.585676	7049.111317	14.861376	-0.057474	4.529670
282.474515	7041.146545	14.866381	-0.057449	4.527195
282.564399	7033.084721	14.871386	-0.057460	4.524688
282.543945	7025.177431	14.876391	-0.057451	4.522228
282.368528	7017.082848	14.881395	-0.057414	4.519708
282.390673	7009.183073	14.886400	-0.057413	4.517247
282.264447	7001.076193	14.891405	-0.057384	4.514721
282.101617	6993.038205	14.896410	-0.057349	4.512214
282.131611	6985.051508	14.901415	-0.057349	4.509722
282.145373	6977.024339	14.906419	-0.057346	4.507217
282.054335	6969.066320	14.911424	-0.057324	4.504731
282.054555	6961.098103	14.916429	-0.057319	4.502241
282.133063	6953.082819	14.921434	-0.057329	4.499735
282.068782	6945.144884	14.926439	-0.057312	4.497251
281.849626	6937.047051	14.931443	-0.057266	4.494716
281.950124	6929.058969	14.936448	-0.057280	4.492214
281.934796	6921.019477	14.941453	-0.057272	4.489695
281.629134	6913.063576	14.946458	-0.057210	4.487199
281.594401	6905.029338	14.951463	-0.057198	4.484679
281.692067	6897.072061	14.956467	-0.057211	4.482181
281.657007	6889.078636	14.961472	-0.057200	4.479670
281.480997	6881.123772	14.966477	-0.057162	4.477170
281.434909	6873.055094	14.971482	-0.057148	4.474633
281.580800	6865.054670	14.976487	-0.057170	4.472116
281.494329	6856.989566	14.981491	-0.057149	4.469577
281.524928	6849.031975	14.986496	-0.057150	4.467070
281.462609	6841.012439	14.991501	-0.057133	4.464543
281.321591	6833.067572	14.996506	-0.057101	4.462037
281.396272	6825.037919	15.001511	-0.057110	4.459504
281.264233	6817.042696	15.006515	-0.057081	4.456980
281.236173	6809.033148	15.011520	-0.057070	4.454449
281.081776	6800.995991	15.016525	-0.057036	4.451909
281.145775	6792.986694	15.021530	-0.057043	4.449376
281.148550	6785.044785	15.026535	-0.057039	4.446863
281.026680	6776.965876	15.031539	-0.057011	4.444305
281.056759	6769.082004	15.036544	-0.057011	4.441808
280.938049	6761.073386	15.041549	-0.056984	4.439269
280.860563	6753.061026	15.046554	-0.056965	4.436728
280.867345	6745.007004	15.051559	-0.056961	4.434172
280.877589	6736.951688	15.056563	-0.056958	4.431614
280.793799	6728.988688	15.061568	-0.056937	4.429084
280.718056	6720.972243	15.066573	-0.056918	4.426536
280.497881	6712.963344	15.071578	-0.056872	4.423988
280.482273	6705.011332	15.076583	-0.056864	4.421457
280.463481	6696.988457	15.081587	-0.056855	4.418902
280.435593	6688.982118	15.086592	-0.056845	4.416351
280.343144	6680.948041	15.091597	-0.056822	4.413790
280.315213	6672.953960	15.096602	-0.056812	4.411240
280.436893	6664.999529	15.101607	-0.056830	4.408701
280.315009	6656.962296	15.106611	-0.056802	4.406134
280.278850	6649.013517	15.111616	-0.056790	4.403594
280.148574	6641.016088	15.116621	-0.056761	4.401037
280.088838	6633.014493	15.121626	-0.056745	4.398477
280.274745	6625.010890	15.126631	-0.056774	4.395916
280.045521	6616.967669	15.131635	-0.056726	4.393338
280.200314	6608.983602	15.136640	-0.056750	4.390781
280.301846	6600.984541	15.141645	-0.056764	4.388216
280.111603	6592.979270	15.146650	-0.056723	4.385647
280.005813	6585.022115	15.151655	-0.056699	4.383092
280.020415	6576.979242	15.156659	-0.056696	4.380508
279.948046	6569.046473	15.161664	-0.056678	4.377958
279.690416	6560.982719	15.166669	-0.056625	4.375363
279.548104	6553.003357	15.171674	-0.056593	4.372795
279.812947	6544.977109	15.176679	-0.056637	4.370212
279.680935	6537.004114	15.181683	-0.056608	4.367643
279.558042	6528.963095	15.186688	-0.056580	4.365050
279.482379	6521.028633	15.191693	-0.056560	4.362490
279.415127	6512.996207	15.196698	-0.056543	4.359897
279.490729	6505.070360	15.201703	-0.056552	4.357338
279.580535	6496.963432	15.206707	-0.056563	4.354719
279.489493	6488.939061	15.211712	-0.056541	4.352124
279.363470	6480.931757	15.216717	-0.056513	4.349533
279.287556	6472.926400	15.221722	-0.056494	4.346941
279.173138	6464.926598	15.226727	-0.056467	4.344349
279.027117	6456.959202	15.231731	-0.056435	4.341766
279.115778	6448.999700	15.236736	-0.056446	4.339185
279.039312	6440.987588	15.241741	-0.056427	4.336585
278.923486	6432.948426	15.246746	-0.056400	4.333974
278.871518	6424.965708	15.251751	-0.056386	4.331380
278.625214	6416.937047	15.256755	-0.056335	4.328769
278.864059	6408.935950	15.261760	-0.056374	4.326168
278.866523	6400.962720	15.266765	-0.056369	4.323573
278.905653	6392.933136	15.271770	-0.056372	4.320958
278.825355	6385.027789	15.276775	-0.056352	4.318382
278.828007	6376.963655	15.281779	-0.056347	4.315752
278.793245	6368.937775	15.286784	-0.056335	4.313134
278.488950	6360.905462	15.291789	-0.056274	4.310509
278.537458	6352.921046	15.296794	-0.056278	4.307901
278.587825	6344.914676	15.301799	-0.056282	4.305285
278.333817	6336.968646	15.306803	-0.056229	4.302684
278.457950	6328.919802	15.311808	-0.056247	4.300051
278.439161	6320.985853	15.316813	-0.056239	4.297453
278.318718	6312.940937	15.321818	-0.056211	4.294816
278.311501	6304.919337	15.326823	-0.056205	4.292186
278.170355	6296.876302	15.331827	-0.056174	4.289547
278.155675	6288.936085	15.336832	-0.056166	4.286940
278.206911	6280.898424	15.341837	-0.056170	4.284300
278.182714	6272.937782	15.346842	-0.056161	4.281684
278.033088	6264.914824	15.351847	-0.056128	4.279044
277.976523	6256.935403	15.356851	-0.056112	4.276418
278.200380	6248.935074	15.361856	-0.056149	4.273785
277.908560	6240.923930	15.366861	-0.056089	4.271144
277.979403	6232.875693	15.371866	-0.056097	4.268491
277.982417	6224.850226	15.376871	-0.056093	4.265843
277.866686	6216.903667	15.381875	-0.056066	4.263219
277.827234	6208.893020	15.386880	-0.056054	4.260573
277.520212	6200.981133	15.391885	-0.055991	4.257956
277.461169	6192.886618	15.396890	-0.055975	4.255278
277.489266	6184.947745	15.401895	-0.055975	4.252651
277.544710	6176.860358	15.406899	-0.055981	4.249974
277.518171	6168.925289	15.411904	-0.055971	4.247345
277.528589	6160.880257	15.416909	-0.055967	4.244677
277.499464	6152.935428	15.421914	-0.055957	4.242041
277.400068	6144.925064	15.426919	-0.055933	4.239382
277.364185	6136.919922	15.431923	-0.055922	4.236722
277.407503	6128.936433	15.436928	-0.055925	4.234069
277.261384	6120.899366	15.441933	-0.055892	4.231395
277.305833	6112.869640	15.446938	-0.055895	4.228723
277.326083	6104.927198	15.451943	-0.055894	4.226078
277.099323	6096.935823	15.456947	-0.055847	4.223413
276.915577	6088.983002	15.461952	-0.055808	4.220760
276.894869	6080.991305	15.466957	-0.055799	4.218094
276.778587	6072.925166	15.471962	-0.055772	4.215400
276.797629	6064.938788	15.476967	-0.055770	4.212732
276.572531	6056.899248	15.481971	-0.055723	4.210042
276.691265	6048.948135	15.486976	-0.055740	4.207384
276.797627	6040.909124	15.491981	-0.055755	4.204694
276.772469	6032.968604	15.496986	-0.055745	4.202035
276.692901	6024.951876	15.501991	-0.055725	4.199347
276.515428	6016.943278	15.506995	-0.055687	4.196660
276.708329	6008.902588	15.512000	-0.055718	4.193964
276.654500	6000.807622	15.517005	-0.055703	4.191245
276.516427	5992.867298	15.522010	-0.055672	4.188576
276.531375	5984.882798	15.527015	-0.055670	4.185891
276.534509	5976.927910	15.532019	-0.055665	4.183215
276.255928	5968.944313	15.537024	-0.055608	4.180525
276.092141	5960.917880	15.542029	-0.055573	4.177819
276.165823	5952.896584	15.547034	-0.055581	4.175116
276.220277	5944.905133	15.552039	-0.055586	4.172421
276.015511	5936.872609	15.557043	-0.055543	4.169708
275.997086	5928.924393	15.562048	-0.055535	4.167023
275.985836	5920.909971	15.567053	-0.055527	4.164315
275.850260	5912.937148	15.572058	-0.055497	4.161617
275.809704	5904.949827	15.577063	-0.055485	4.158913
275.795854	5896.884809	15.582067	-0.055477	4.156182
275.724208	5888.887822	15.587072	-0.055458	4.153472
275.686041	5880.869197	15.592077	-0.055446	4.150753
275.760493	5872.867690	15.597082	-0.055455	4.148039
275.731913	5864.886841	15.602087	-0.055445	4.145329
275.675429	5856.899321	15.607091	-0.055429	4.142614
275.754051	5848.873873	15.612096	-0.055438	4.139887
275.568147	5840.946304	15.617101	-0.055399	4.137188
275.540086	5832.891991	15.622106	-0.055388	4.134446
275.369033	5824.913081	15.627111	-0.055352	4.131726
275.355415	5816.841502	15.632115	-0.055344	4.128975
275.231079	5808.883534	15.637120	-0.055316	4.126259
275.156570	5800.940983	15.642125	-0.055297	4.123547
275.273668	5792.910962	15.647130	-0.055313	4.120806
275.223869	5784.929670	15.652135	-0.055299	4.118078
275.057908	5776.910431	15.657139	-0.055263	4.115333
275.188963	5768.874904	15.662144	-0.055282	4.112585
275.084945	5760.837778	15.667149	-0.055258	4.109831
274.886768	5752.861453	15.672154	-0.055216	4.107095
274.928032	5744.880799	15.677159	-0.055219	4.104359
274.952807	5736.880601	15.682163	-0.055218	4.101614
274.886592	5728.896415	15.687168	-0.055201	4.098872
274.798022	5720.899369	15.692173	-0.055179	4.096123
274.837249	5712.872065	15.697178	-0.055181	4.093364
274.924131	5704.911859	15.702183	-0.055192	4.090626
274.760911	5696.873095	15.707187	-0.055157	4.087856
274.474943	5688.911579	15.712192	-0.055099	4.085109
274.594401	5680.940876	15.717197	-0.055116	4.082363
274.661999	5672.951263	15.722202	-0.055123	4.079607
274.681973	5664.960738	15.727207	-0.055122	4.076849
274.399949	5656.927771	15.732211	-0.055064	4.074070
274.523808	5648.926934	15.737216	-0.055082	4.071306
274.555581	5640.926092	15.742221	-0.055083	4.068539
274.373115	5632.899499	15.747226	-0.055044	4.065758
274.630763	5624.975395	15.752231	-0.055087	4.063016
274.459785	5616.922415	15.757235	-0.055050	4.060222
274.300573	5608.973552	15.762240	-0.055015	4.057463
274.284129	5600.923711	15.767245	-0.055007	4.054668
274.146489	5592.919388	15.772250	-0.054976	4.051886
274.132943	5584.946996	15.777255	-0.054969	4.049115
274.148609	5576.929531	15.782259	-0.054966	4.046326
274.143092	5568.946260	15.787264	-0.054960	4.043547
273.861146	5560.951241	15.792269	-0.054903	4.040758
273.772750	5552.971736	15.797274	-0.054881	4.037976
273.977076	5544.967666	15.802279	-0.054914	4.035187
273.840085	5536.815266	15.807283	-0.054884	4.032339
273.643997	5528.863278	15.812288	-0.054842	4.029559
273.594522	5520.864235	15.817293	-0.054828	4.026762
273.620018	5512.845284	15.822298	-0.054827	4.023957
273.728069	5504.914881	15.827303	-0.054842	4.021183
273.689603	5496.914226	15.832307	-0.054830	4.018380
273.583267	5488.940799	15.837312	-0.054805	4.015584
273.526494	5480.893423	15.842317	-0.054790	4.012760
273.384450	5472.859897	15.847322	-0.054758	4.009938
273.492729	5464.939329	15.852327	-0.054773	4.007158
273.321472	5456.913956	15.857331	-0.054736	4.004334
273.340948	5448.938266	15.862336	-0.054735	4.001529
273.305529	5440.950204	15.867341	-0.054723	3.998717
273.250218	5432.911964	15.872346	-0.054708	3.995885
273.085072	5424.914462	15.877351	-0.054672	3.993063
272.876043	5416.909616	15.882355	-0.054628	3.990236
272.952080	5408.911843	15.887360	-0.054637	3.987414
272.998036	5400.885728	15.892365	-0.054640	3.984580
272.760356	5392.930289	15.897370	-0.054591	3.981764
273.006581	5384.939093	15.902375	-0.054632	3.978941
272.945575	5376.941103	15.907379	-0.054615	3.976108
272.863049	5368.931334	15.912384	-0.054595	3.973270
272.837597	5360.902686	15.917389	-0.054585	3.970423
272.598672	5352.951301	15.922394	-0.054535	3.967598
272.611939	5344.960527	15.927399	-0.054533	3.964761
272.511191	5336.992230	15.932403	-0.054509	3.961929
272.575974	5328.961331	15.937408	-0.054516	3.959075
272.444946	5320.998953	15.942413	-0.054486	3.956240
272.373349	5312.943108	15.947418	-0.054468	3.953370
272.269360	5304.927975	15.952423	-0.054443	3.950513
272.244717	5296.952538	15.957427	-0.054434	3.947668
272.292084	5288.949673	15.962432	-0.054438	3.944814
272.077639	5280.987924	15.967437	-0.054393	3.941967
271.961621	5272.951281	15.972442	-0.054366	3.939093
272.058808	5265.003587	15.977447	-0.054379	3.936253
272.029716	5256.989263	15.982451	-0.054368	3.933384
272.009625	5248.955964	15.987456	-0.054359	3.930507
271.923589	5241.005823	15.992461	-0.054338	3.927656
271.959668	5232.957141	15.997466	-0.054340	3.924770
272.154003	5225.008267	16.002471	-0.054371	3.921921
271.950936	5216.984065	16.007475	-0.054328	3.919035
271.823533	5209.011579	16.012480	-0.054299	3.916167
271.675070	5201.015684	16.017485	-0.054267	3.913289
271.723995	5192.942117	16.022490	-0.054271	3.910383
271.764518	5184.993648	16.027495	-0.054273	3.907521
271.634921	5176.959199	16.032499	-0.054244	3.904622
271.592167	5169.031030	16.037504	-0.054231	3.901761
271.651487	5160.996296	16.042509	-0.054237	3.898861
271.488890	5152.989270	16.047514	-0.054201	3.895965
271.715318	5144.980327	16.052519	-0.054239	3.893074
271.603038	5136.983537	16.057523	-0.054213	3.890178
271.275421	5129.042711	16.062528	-0.054146	3.887296
271.167473	5121.020696	16.067533	-0.054121	3.884387
271.198937	5112.995735	16.072538	-0.054122	3.881478
271.162686	5105.028491	16.077543	-0.054110	3.878585
270.982852	5096.998301	16.082547	-0.054072	3.875665
270.993850	5088.795016	16.087552	-0.054068	3.872684
270.946468	5080.826785	16.092557	-0.054055	3.869784
270.751390	5072.892993	16.097562	-0.054013	3.866893
270.802538	5064.895528	16.102567	-0.054018	3.863980
270.854615	5056.916867	16.107571	-0.054022	3.861072
270.877115	5048.990272	16.112576	-0.054021	3.858181
270.789392	5040.953347	16.117581	-0.054000	3.855244
270.695486	5032.998936	16.122586	-0.053977	3.852336
270.640398	5025.009210	16.127591	-0.053962	3.849413
270.471839	5016.976350	16.132595	-0.053926	3.846470
270.625730	5009.010438	16.137600	-0.053949	3.843556
270.502089	5001.041082	16.142605	-0.053921	3.840632
270.375857	4993.055874	16.147610	-0.053892	3.837701
270.584291	4985.053191	16.152615	-0.053926	3.834767
270.509180	4976.998402	16.157619	-0.053907	3.831807
270.452888	4969.015886	16.162624	-0.053891	3.828871
270.380676	4961.015818	16.167629	-0.053873	3.825926
270.371210	4953.053171	16.172634	-0.053866	3.822993
270.360756	4945.088231	16.177639	-0.053859	3.820058
270.289625	4937.078697	16.182643	-0.053841	3.817103
270.370660	4929.067612	16.187648	-0.053851	3.814148
270.281479	4921.065642	16.192653	-0.053829	3.811190
270.065502	4913.084772	16.197658	-0.053784	3.808236
270.147990	4905.077897	16.202663	-0.053794	3.805275
269.974596	4897.108805	16.207667	-0.053757	3.802321
269.917772	4889.091248	16.212672	-0.053741	3.799350
269.808706	4881.134360	16.217677	-0.053716	3.796397
269.805127	4873.053964	16.222682	-0.053710	3.793398
269.848718	4865.067125	16.227687	-0.053713	3.790433
269.699080	4857.070123	16.232691	-0.053680	3.787457
269.723849	4849.056653	16.237696	-0.053679	3.784477
269.677681	4841.115705	16.242701	-0.053666	3.781520
269.431425	4833.103191	16.247706	-0.053615	3.778529
269.573562	4825.097539	16.252711	-0.053636	3.775547
269.408362	4817.070443	16.257715	-0.053600	3.772548
269.428308	4809.057978	16.262720	-0.053599	3.769557
269.325456	4801.136878	16.267725	-0.053575	3.766594
269.257239	4793.103176	16.272730	-0.053557	3.763587
269.274128	4785.118318	16.277735	-0.053555	3.760599
269.171213	4777.125393	16.282739	-0.053531	3.757602
269.387130	4769.065453	16.287744	-0.053566	3.754585
269.171127	4761.107216	16.292749	-0.053521	3.751594
269.145481	4753.066524	16.297754	-0.053511	3.748573
268.899668	4745.129677	16.302759	-0.053460	3.745585
268.996862	4737.135060	16.307763	-0.053473	3.742580
268.963832	4729.130814	16.312768	-0.053462	3.739566
268.811277	4721.166110	16.317773	-0.053428	3.736561
268.894744	4713.096411	16.322778	-0.053438	3.733521
269.033311	4705.122447	16.327783	-0.053459	3.730515
268.656946	4697.149814	16.332787	-0.053384	3.727495
268.567521	4689.157590	16.337792	-0.053362	3.724472
268.749353	4681.173013	16.342797	-0.053391	3.721456
268.797704	4673.173570	16.347802	-0.053395	3.718428
268.692463	4665.224101	16.352807	-0.053370	3.715414
268.667259	4657.079381	16.357811	-0.053360	3.712324
268.651656	4649.103653	16.362816	-0.053353	3.709297
268.392292	4641.131102	16.367821	-0.053299	3.706262
268.340584	4633.141243	16.372826	-0.053284	3.703224
268.415191	4625.177752	16.377831	-0.053293	3.700196
268.128537	4617.217781	16.382835	-0.053235	3.697158
268.254871	4609.191146	16.387840	-0.053253	3.694102
268.186858	4601.166506	16.392845	-0.053235	3.691040
267.868950	4593.206487	16.397850	-0.053171	3.687993
267.936339	4585.201952	16.402855	-0.053179	3.684937
267.851052	4577.247472	16.407859	-0.053158	3.681893
268.083059	4569.246199	16.412864	-0.053196	3.678837
267.978692	4561.241813	16.417869	-0.053171	3.675769
267.534741	4553.229916	16.422874	-0.053084	3.672686
267.871185	4545.210762	16.427879	-0.053141	3.669618
267.711365	4537.233521	16.432883	-0.053106	3.666551
267.783369	4529.242741	16.437888	-0.053115	3.663482
267.784025	4521.239859	16.442893	-0.053110	3.660404
267.680583	4513.255543	16.447898	-0.053085	3.657328
267.550510	4505.282214	16.452903	-0.053056	3.654253
267.441532	4497.225214	16.457907	-0.053031	3.651143
267.432512	4489.254911	16.462912	-0.053024	3.648067
267.219440	4481.259907	16.467917	-0.052979	3.644974
267.186908	4473.285368	16.472922	-0.052968	3.641890
267.406334	4465.285932	16.477927	-0.053004	3.638801
267.302494	4457.280614	16.482931	-0.052979	3.635698
267.276027	4449.242261	16.487936	-0.052969	3.632582
267.115981	4441.247348	16.492941	-0.052934	3.629477
267.014161	4433.233643	16.497946	-0.052910	3.626363
266.980246	4425.302496	16.502951	-0.052899	3.623280
266.734474	4417.301312	16.507955	-0.052848	3.620162
266.874261	4409.308424	16.512960	-0.052869	3.617055
266.878858	4401.302124	16.517965	-0.052865	3.613936
266.873662	4393.294618	16.522970	-0.052859	3.610813
266.848365	4385.333839	16.527975	-0.052849	3.607706
266.664700	4377.305566	16.532979	-0.052810	3.604565
266.779199	4369.359175	16.537984	-0.052826	3.601462
266.510360	4361.369290	16.542989	-0.052771	3.598329
266.364538	4353.352282	16.547994	-0.052738	3.595185
266.298593	4345.358182	16.552999	-0.052721	3.592050
266.336304	4337.337465	16.558003	-0.052723	3.588904
266.366412	4329.333055	16.563008	-0.052724	3.585762
266.172218	4321.393796	16.568013	-0.052682	3.582637
266.160088	4313.361216	16.573018	-0.052675	3.579477
266.336740	4305.426787	16.578023	-0.052703	3.576359
266.271284	4297.397878	16.583027	-0.052685	3.573193
266.260611	4289.383232	16.588032	-0.052678	3.570032
266.019063	4281.432769	16.593037	-0.052628	3.566887
265.918147	4273.400212	16.598042	-0.052604	3.563711
266.125320	4265.436044	16.603047	-0.052638	3.560568
266.010839	4257.439271	16.608051	-0.052612	3.557399
266.005028	4249.405470	16.613056	-0.052605	3.554217
266.082361	4241.336555	16.618061	-0.052615	3.551020
265.611516	4233.381350	16.623066	-0.052522	3.547849
265.753400	4225.373250	16.628071	-0.052543	3.544673
265.644402	4217.419123	16.633075	-0.052518	3.541507
265.563125	4209.441871	16.638080	-0.052498	3.538330
265.575838	4201.429561	16.643085	-0.052495	3.535140
265.333314	4193.428681	16.648090	-0.052445	3.531943
265.468998	4185.440461	16.653095	-0.052465	3.528760
265.282268	4177.419530	16.658099	-0.052425	3.525551
265.330622	4169.464019	16.663104	-0.052429	3.522373
265.496254	4161.452219	16.668109	-0.052455	3.519172
265.128093	4153.523104	16.673114	-0.052381	3.515986
265.427837	4145.480600	16.678119	-0.052432	3.512772
265.339665	4137.429720	16.683123	-0.052410	3.509539
265.109353	4129.480297	16.688128	-0.052362	3.506340
265.012000	4121.500123	16.693133	-0.052339	3.503130
265.044049	4113.457664	16.698138	-0.052340	3.499895
265.153552	4105.561600	16.703143	-0.052355	3.496719
264.883176	4097.531593	16.708147	-0.052300	3.493474
264.939435	4089.511019	16.713152	-0.052305	3.490241
264.899260	4081.571790	16.718157	-0.052293	3.487034
264.527754	4073.580677	16.723162	-0.052218	3.483793
264.577696	4065.598318	16.728167	-0.052223	3.480565
264.495236	4057.614408	16.733171	-0.052202	3.477330
264.541996	4049.605536	16.738176	-0.052206	3.474085
264.503226	4041.564681	16.743181	-0.052193	3.470822
264.442789	4033.576151	16.748186	-0.052177	3.467577
264.554693	4025.585390	16.753191	-0.052193	3.464332
264.297250	4017.602865	16.758195	-0.052140	3.461077
264.375313	4009.617497	16.763200	-0.052149	3.457828
264.292081	4001.585034	16.768205	-0.052129	3.454551
264.172192	3993.591453	16.773210	-0.052101	3.451286
264.157684	3985.624601	16.778215	-0.052094	3.448032
264.186186	3977.607635	16.783219	-0.052094	3.444757
264.240193	3969.676328	16.788224	-0.052099	3.441513
264.076853	3961.671646	16.793229	-0.052063	3.438230
263.892783	3953.654285	16.798234	-0.052024	3.434938
263.937541	3945.671094	16.803239	-0.052027	3.431664
264.053082	3937.644188	16.808243	-0.052044	3.428371
263.820985	3929.680479	16.813248	-0.051995	3.425089
263.730727	3921.716770	16.818253	-0.051973	3.421809
263.621073	3913.710808	16.823258	-0.051948	3.418508
263.565334	3905.749857	16.828263	-0.051932	3.415224
263.632804	3897.699544	16.833267	-0.051940	3.411904
263.803571	3889.687837	16.838272	-0.051967	3.408600
263.395007	3881.775281	16.843277	-0.051885	3.405315
263.457573	3873.763830	16.848282	-0.051892	3.402001
263.447086	3865.793317	16.853287	-0.051885	3.398699
263.327245	3857.793724	16.858291	-0.051858	3.395377
263.068357	3849.715099	16.863296	-0.051804	3.392015
263.334353	3841.711287	16.868301	-0.051849	3.388698
262.986488	3833.746933	16.873306	-0.051779	3.385374
262.959216	3825.796721	16.878311	-0.051769	3.382063
263.166759	3817.786695	16.883315	-0.051802	3.378732
263.053041	3809.804002	16.888320	-0.051776	3.375398
262.903909	3801.804589	16.893325	-0.051743	3.372052
262.825720	3793.798239	16.898330	-0.051723	3.368703
263.124703	3785.808238	16.903335	-0.051774	3.365371
262.803030	3777.845892	16.908339	-0.051709	3.362024
262.808908	3769.877916	16.913344	-0.051705	3.358684
262.732909	3761.904770	16.918349	-0.051686	3.355336
262.882626	3753.828974	16.923354	-0.051709	3.351948
262.649700	3745.877892	16.928359	-0.051660	3.348597
262.575700	3737.872319	16.933363	-0.051641	3.345224
262.658688	3729.894680	16.938368	-0.051652	3.341866
262.591557	3721.902456	16.943373	-0.051634	3.338493
262.275963	3713.939815	16.948378	-0.051570	3.335119
262.498800	3705.916605	16.953383	-0.051607	3.331737
262.295566	3697.910395	16.958387	-0.051564	3.328342
262.159322	3689.933889	16.963392	-0.051533	3.324959
262.216792	3681.993581	16.968397	-0.051539	3.321595
262.075275	3673.981619	16.973402	-0.051507	3.318190
262.261469	3665.985982	16.978407	-0.051537	3.314800
262.124873	3657.952654	16.983411	-0.051506	3.311379
262.104293	3649.954145	16.988416	-0.051498	3.307974
261.872126	3641.995722	16.993421	-0.051449	3.304574
261.645402	3634.009278	16.998426	-0.051402	3.301159
261.838948	3626.038573	17.003431	-0.051433	3.297763
261.706664	3618.038475	17.008435	-0.051403	3.294338
261.494029	3610.045887	17.013440	-0.051359	3.290910
261.578023	3602.065162	17.018445	-0.051369	3.287495
261.712939	3594.034291	17.023450	-0.051389	3.284057
261.591424	3586.100881	17.028455	-0.051361	3.280647
261.260023	3578.156124	17.033459	-0.051295	3.277221
261.328036	3570.107752	17.038464	-0.051302	3.273761
261.293329	3562.088710	17.043469	-0.051291	3.270307
261.139118	3554.110670	17.048474	-0.051257	3.266862
261.349777	3546.116057	17.053479	-0.051291	3.263421
261.214413	3538.135155	17.058483	-0.051261	3.259968
261.227130	3530.181791	17.063488	-0.051258	3.256530
261.222838	3522.140339	17.068493	-0.051252	3.253049
260.983732	3514.136134	17.073498	-0.051202	3.249571
260.955433	3506.194704	17.078503	-0.051192	3.246125
261.027888	3498.179916	17.083507	-0.051201	3.242647
260.856241	3490.228418	17.088512	-0.051164	3.239184
260.942528	3482.251011	17.093517	-0.051175	3.235715
260.600420	3474.184126	17.098522	-0.051106	3.232187
260.695421	3466.187401	17.103527	-0.051118	3.228703
260.596800	3458.180040	17.108531	-0.051095	3.225203
260.476046	3450.254153	17.113536	-0.051067	3.221734
260.525936	3442.248964	17.118541	-0.051071	3.218233
260.477322	3434.250964	17.123546	-0.051057	3.214728
260.551099	3426.270203	17.128551	-0.051066	3.211231
260.592570	3418.252793	17.133555	-0.051069	3.207714
260.449764	3410.294819	17.138560	-0.051037	3.204210
260.392689	3402.334016	17.143565	-0.051021	3.200706
260.489272	3394.334192	17.148570	-0.051034	3.197186
260.333319	3386.345033	17.153575	-0.051000	3.193657
260.301079	3378.339653	17.158579	-0.050989	3.190122
260.102508	3370.385763	17.163584	-0.050947	3.186599
260.371370	3362.363928	17.168589	-0.050992	3.183061
260.101028	3354.391633	17.173594	-0.050936	3.179519
259.837169	3346.460817	17.178599	-0.050882	3.175991
259.821465	3338.409085	17.183603	-0.050874	3.172417
259.923801	3330.404988	17.188608	-0.050888	3.168864
259.865181	3322.436486	17.193613	-0.050872	3.165317
259.790570	3314.470781	17.198618	-0.050853	3.161766
259.894448	3306.497567	17.203623	-0.050868	3.158215
259.590958	3298.512485	17.208627	-0.050806	3.154638
259.511257	3290.481454	17.213632	-0.050786	3.151045
259.506509	3282.495597	17.218637	-0.050780	3.147472
259.329880	3274.493016	17.223642	-0.050742	3.143880
259.470864	3266.532080	17.228647	-0.050763	3.140316
259.252719	3258.542157	17.233651	-0.050718	3.136719
259.271967	3250.564001	17.238656	-0.050716	3.133134
259.152376	3242.567650	17.243661	-0.050689	3.129531
259.101857	3234.575181	17.248666	-0.050674	3.125928
259.154369	3226.621952	17.253671	-0.050679	3.122344
259.022457	3218.635187	17.258675	-0.050649	3.118731
258.957435	3210.639410	17.263680	-0.050632	3.115114
258.878508	3202.634338	17.268685	-0.050612	3.111487
258.912409	3194.639169	17.273690	-0.050613	3.107866
258.837527	3186.683360	17.278695	-0.050594	3.104254
258.539809	3178.695814	17.283699	-0.050534	3.100613
258.836563	3170.699044	17.288704	-0.050584	3.096990
258.766132	3162.691947	17.293709	-0.050566	3.093341
258.424960	3154.701570	17.298714	-0.050497	3.089684
258.776071	3146.713654	17.303719	-0.050558	3.086055
258.781392	3138.732809	17.308723	-0.050554	3.082409
258.420458	3130.805085	17.313728	-0.050481	3.078766
258.476266	3122.808118	17.318733	-0.050487	3.075107
258.473914	3114.699266	17.323738	-0.050481	3.071389
258.403864	3106.770212	17.328743	-0.050463	3.067746
258.218386	3098.788322	17.333747	-0.050423	3.064069
258.228035	3090.805777	17.338752	-0.050420	3.060396
258.277587	3082.845004	17.343757	-0.050424	3.056731
258.260072	3074.831600	17.348762	-0.050416	3.053034
258.160860	3066.873421	17.353767	-0.050392	3.049354
258.156021	3058.868678	17.358771	-0.050386	3.045652
258.114980	3050.915126	17.363776	-0.050374	3.041968
258.033039	3042.955241	17.368781	-0.050353	3.038275
258.061461	3034.931188	17.373786	-0.050353	3.034553
258.102161	3026.924431	17.378791	-0.050356	3.030834
257.553021	3018.988445	17.383795	-0.050249	3.027116
257.619774	3011.000727	17.388800	-0.050256	3.023399
257.812014	3002.999077	17.393805	-0.050287	3.019676
257.645210	2995.033824	17.398810	-0.050251	3.015949
257.689635	2987.033152	17.403815	-0.050254	3.012211
257.631303	2979.019784	17.408819	-0.050238	3.008457
257.539617	2971.037244	17.413824	-0.050216	3.004711
257.385742	2963.113108	17.418829	-0.050182	3.000985
257.187901	2955.130462	17.423834	-0.050140	2.997224
257.412349	2947.110899	17.428839	-0.050177	2.993463
257.224191	2939.093749	17.433843	-0.050137	2.989677
256.996654	2931.137314	17.438848	-0.050089	2.985913
257.256592	2923.150079	17.443853	-0.050132	2.982154
257.137985	2915.171953	17.448858	-0.050105	2.978376
257.078292	2907.218193	17.453863	-0.050089	2.974607
257.093929	2899.194141	17.458867	-0.050087	2.970804
256.936516	2891.225074	17.463872	-0.050052	2.967014
256.875841	2883.259894	17.468877	-0.050036	2.963225
256.859623	2875.272646	17.473882	-0.050028	2.959424
256.838317	2867.324372	17.478887	-0.050019	2.955635
256.748323	2859.300151	17.483891	-0.049997	2.951803
256.724015	2851.296324	17.488896	-0.049988	2.947978
256.848273	2843.316258	17.493901	-0.050006	2.944167
256.617382	2835.360002	17.498906	-0.049958	2.940345
256.531795	2827.408928	17.503911	-0.049937	2.936527
256.466794	2819.399742	17.508915	-0.049919	2.932678
256.422846	2811.408556	17.513920	-0.049906	2.928833
256.311032	2803.443035	17.518925	-0.049880	2.924992
256.312227	2795.458268	17.523930	-0.049875	2.921142
256.359819	2787.503527	17.528935	-0.049879	2.917305
256.293692	2779.456759	17.533939	-0.049862	2.913412
255.981822	2771.440575	17.538944	-0.049799	2.909515
256.096366	2763.474180	17.543949	-0.049815	2.905660
256.179805	2755.494712	17.548954	-0.049825	2.901792
256.236044	2747.532040	17.553959	-0.049831	2.897925
255.941313	2739.596835	17.558963	-0.049771	2.894048
255.718437	2731.573573	17.563968	-0.049724	2.890127
255.953349	2723.595748	17.568973	-0.049763	2.886246
255.898871	2715.619071	17.573978	-0.049748	2.882346
255.838034	2707.677519	17.578983	-0.049731	2.878457
255.778115	2699.675945	17.583987	-0.049715	2.874534
255.734094	2691.682922	17.588992	-0.049702	2.870610
255.657329	2683.703868	17.593997	-0.049682	2.866686
255.572492	2675.725901	17.599002	-0.049661	2.862757
255.527875	2667.775965	17.604007	-0.049648	2.858838
255.443785	2659.778767	17.609011	-0.049627	2.854888
255.595821	2651.759214	17.614016	-0.049650	2.850935
255.511762	2643.813213	17.619021	-0.049630	2.847000
255.144283	2635.869248	17.624026	-0.049556	2.843045
255.169823	2627.912294	17.629031	-0.049556	2.839099
255.052546	2619.928525	17.634035	-0.049529	2.835126
254.912129	2611.916611	17.639040	-0.049498	2.831133
254.908541	2603.921217	17.644045	-0.049492	2.827150
254.921397	2595.928344	17.649050	-0.049489	2.823164
255.056243	2587.947225	17.654055	-0.049509	2.819184
255.057271	2579.972608	17.659059	-0.049505	2.815195
254.824253	2571.995557	17.664064	-0.049456	2.811185
254.781411	2564.039962	17.669069	-0.049443	2.807192
254.629773	2556.067822	17.674074	-0.049410	2.803178
254.766305	2548.084011	17.679079	-0.049430	2.799169
254.697202	2540.124071	17.684083	-0.049412	2.795154
254.553542	2532.118038	17.689088	-0.049380	2.791106
254.496887	2524.149465	17.694093	-0.049365	2.787076
254.344113	2516.180134	17.699098	-0.049331	2.783035
254.486184	2508.200628	17.704103	-0.049353	2.778999
254.347147	2500.236353	17.709107	-0.049322	2.774949
254.188125	2492.248048	17.714112	-0.049287	2.770879
254.232597	2484.286493	17.719117	-0.049290	2.766830
254.160685	2476.298118	17.724122	-0.049272	2.762753
254.246870	2468.327552	17.729127	-0.049283	2.758689
254.096056	2460.359794	17.734131	-0.049249	2.754607
253.979307	2452.284787	17.739136	-0.049223	2.750465
253.932476	2444.331214	17.744141	-0.049209	2.746384
253.921372	2436.350056	17.749146	-0.049202	2.742284
253.803401	2428.429814	17.754151	-0.049175	2.738203
253.713377	2420.451527	17.759155	-0.049153	2.734088
253.682223	2412.449924	17.764160	-0.049142	2.729958
253.432367	2404.530404	17.769165	-0.049090	2.725851
253.472777	2396.531880	17.774170	-0.049093	2.721715
253.560066	2388.567615	17.779175	-0.049104	2.717593
253.505985	2380.582307	17.784179	-0.049089	2.713445
253.504313	2372.578389	17.789184	-0.049083	2.709284
253.598745	2364.609453	17.794189	-0.049096	2.705142
253.545505	2356.638009	17.799194	-0.049081	2.700982
253.397728	2348.723045	17.804199	-0.049048	2.696839
253.135746	2340.735007	17.809203	-0.048994	2.692645
253.261321	2332.723146	17.814208	-0.049013	2.688456
253.467270	2324.741975	17.819213	-0.049046	2.684281
253.058661	2316.819832	17.824218	-0.048965	2.680093
252.953678	2308.871295	17.829223	-0.048940	2.675902
252.884452	2300.841585	17.834227	-0.048922	2.671665
252.758533	2292.856921	17.839232	-0.048894	2.667442
252.805793	2284.884620	17.844237	-0.048898	2.663229
252.793970	2276.906754	17.849242	-0.048890	2.659002
252.760441	2268.962444	17.854247	-0.048879	2.654786
252.656181	2260.957197	17.859251	-0.048854	2.650526
252.580517	2253.007987	17.864256	-0.048835	2.646290
252.782750	2245.032895	17.869261	-0.048868	2.642052
252.470253	2237.091134	17.874266	-0.048805	2.637792
252.575884	2229.103822	17.879271	-0.048819	2.633527
252.378068	2221.121515	17.884275	-0.048777	2.629238
252.217147	2213.151877	17.889280	-0.048742	2.624952
252.259662	2205.210626	17.894285	-0.048745	2.620687
252.297537	2197.217650	17.899290	-0.048747	2.616387
252.185993	2189.249890	17.904295	-0.048721	2.612084
252.152778	2181.268588	17.909299	-0.048710	2.607771
251.906575	2173.323161	17.914304	-0.048659	2.603457
252.007201	2165.358631	17.919309	-0.048673	2.599148
251.761613	2157.402312	17.924314	-0.048622	2.594813
251.759617	2149.221390	17.929319	-0.048616	2.590365
251.798554	2141.261905	17.934323	-0.048619	2.586033
251.816716	2133.332335	17.939328	-0.048617	2.581708
251.724046	2125.421343	17.944333	-0.048595	2.577379
251.672902	2117.457510	17.949338	-0.048580	2.573017
251.665326	2109.493774	17.954343	-0.048574	2.568650
251.517495	2101.526854	17.959347	-0.048541	2.564264
251.503108	2093.577822	17.964352	-0.048533	2.559890
251.307030	2085.675201	17.969357	-0.048492	2.555521
251.379690	2077.646600	17.974362	-0.048500	2.551094
251.470686	2069.663973	17.979367	-0.048512	2.546686
251.487357	2061.696078	17.984371	-0.048510	2.542273
251.214397	2053.775663	17.989376	-0.048454	2.537858
251.169478	2045.814957	17.994381	-0.048441	2.533430
251.198915	2037.800196	17.999386	-0.048441	2.528969
251.295943	2029.853001	18.004391	-0.048454	2.524542
251.020762	2021.930919	18.009395	-0.048398	2.520095
250.911330	2013.981174	18.014400	-0.048372	2.515637
250.898454	2005.967034	18.019405	-0.048365	2.511141
250.757268	1997.995362	18.024410	-0.048334	2.506652
250.730623	1990.045505	18.029415	-0.048324	2.502176
250.708582	1982.067804	18.034419	-0.048314	2.497676
250.700913	1974.108157	18.039424	-0.048308	2.493179
250.706490	1966.143797	18.044429	-0.048304	2.488673
250.483341	1958.183797	18.049434	-0.048257	2.484144
250.658029	1950.211671	18.054439	-0.048285	2.479629
250.474218	1942.285067	18.059443	-0.048245	2.475105
250.505391	1934.275665	18.064448	-0.048246	2.470541
250.426456	1926.325388	18.069453	-0.048226	2.465995
250.460191	1918.347615	18.074458	-0.048228	2.461433
250.159202	1910.456271	18.079463	-0.048166	2.456887
250.128117	1902.457570	18.084467	-0.048156	2.452291
250.015846	1894.488016	18.089472	-0.048130	2.447697
249.985873	1886.545975	18.094477	-0.048119	2.443117
249.992980	1878.571312	18.099482	-0.048115	2.438512
250.014371	1870.617100	18.104487	-0.048114	2.433911
249.801839	1862.587898	18.109491	-0.048069	2.429240
249.572934	1854.648109	18.114496	-0.048022	2.424611
249.850477	1846.683329	18.119501	-0.048068	2.419997
249.885312	1838.720689	18.124506	-0.048070	2.415357
249.673751	1830.773358	18.129511	-0.048025	2.410698
249.609810	1822.805437	18.134515	-0.048008	2.406029
249.504330	1814.871822	18.139520	-0.047984	2.401368
249.591360	1806.921713	18.144525	-0.047995	2.396703
249.342412	1798.959956	18.149530	-0.047943	2.391996
249.345218	1790.978878	18.154535	-0.047939	2.387288
249.403058	1783.022808	18.159539	-0.047945	2.382590
248.966612	1775.120026	18.164544	-0.047858	2.377875
249.057592	1767.156537	18.169549	-0.047870	2.373156
248.969928	1759.162747	18.174554	-0.047849	2.368396
248.857564	1751.227389	18.179559	-0.047823	2.363659
248.944449	1743.266323	18.184563	-0.047834	2.358913
248.727448	1735.331371	18.189568	-0.047788	2.354149
248.763962	1727.337846	18.194573	-0.047790	2.349360
248.515657	1719.372049	18.199578	-0.047739	2.344555
248.650789	1711.421398	18.204583	-0.047759	2.339781
248.733913	1703.464704	18.209587	-0.047769	2.334989
248.629775	1695.491880	18.214592	-0.047745	2.330161
248.712836	1687.553208	18.219597	-0.047755	2.325360
248.617835	1679.597271	18.224602	-0.047733	2.320524
248.419614	1671.700492	18.229607	-0.047691	2.315705
248.274703	1663.715256	18.234611	-0.047659	2.310827
248.219535	1655.763307	18.239616	-0.047643	2.305966
248.188203	1647.820304	18.244621	-0.047632	2.301102
247.886225	1639.889735	18.249626	-0.047571	2.296213
248.238769	1631.881642	18.254631	-0.047632	2.291321
247.899427	1623.959877	18.259635	-0.047563	2.286413
247.593315	1616.035106	18.264640	-0.047501	2.281495
247.847325	1608.072637	18.269645	-0.047544	2.276591
247.788972	1600.050252	18.274650	-0.047528	2.271613
247.537757	1592.107259	18.279655	-0.047476	2.266657
247.523686	1584.157758	18.284659	-0.047468	2.261706
247.537254	1576.208337	18.289664	-0.047466	2.256746
247.609092	1568.249834	18.294669	-0.047474	2.251775
247.397629	1560.304416	18.299674	-0.047429	2.246777
247.549024	1552.363067	18.304679	-0.047453	2.241801
247.465673	1544.431809	18.309683	-0.047432	2.236801
247.135741	1536.508746	18.314688	-0.047366	2.231772
247.333984	1528.521095	18.319693	-0.047397	2.226738
247.247197	1520.583601	18.324698	-0.047376	2.221699
247.028173	1512.687347	18.329703	-0.047330	2.216663
246.966573	1504.717061	18.334707	-0.047314	2.211583
247.154216	1496.733771	18.339712	-0.047344	2.206504
247.139200	1488.822323	18.344717	-0.047336	2.201442
246.870403	1480.910099	18.349722	-0.047281	2.196345
246.641015	1472.958455	18.354727	-0.047233	2.191214
246.701271	1464.978380	18.359731	-0.047239	2.186079
246.726806	1457.030599	18.364736	-0.047239	2.180949
246.601215	1449.124331	18.369741	-0.047210	2.175821
246.431219	1441.164967	18.374746	-0.047174	2.170642
246.632942	1433.193491	18.379751	-0.047206	2.165476
246.597596	1425.267171	18.384755	-0.047195	2.160306
246.506589	1417.352727	18.389760	-0.047173	2.155126
246.398938	1409.402843	18.394765	-0.047147	2.149909
246.105124	1401.482753	18.399770	-0.047088	2.144682
246.253441	1393.537664	18.404775	-0.047110	2.139466
246.317481	1385.583954	18.409779	-0.047117	2.134224
246.027402	1377.659478	18.414784	-0.047058	2.128955
245.954499	1369.737271	18.419789	-0.047039	2.123695
245.769028	1361.820654	18.424794	-0.047000	2.118415
245.848210	1353.845087	18.429799	-0.047010	2.113108
245.500264	1345.896441	18.434803	-0.046940	2.107764
245.588390	1337.925267	18.439808	-0.046951	2.102434
245.652891	1330.012230	18.444813	-0.046958	2.097127
245.744883	1322.044310	18.449818	-0.046970	2.091772
245.637542	1314.125821	18.454823	-0.046945	2.086417
245.602991	1306.204254	18.459827	-0.046934	2.081054
245.414083	1298.304172	18.464832	-0.046893	2.075676
245.424576	1290.350060	18.469837	-0.046890	2.070267
245.392298	1282.407621	18.474842	-0.046879	2.064847
245.369487	1274.500158	18.479847	-0.046870	2.059438
245.251868	1266.584108	18.484851	-0.046843	2.054000
245.248328	1258.627270	18.489856	-0.046837	2.048530
245.190914	1250.718328	18.494861	-0.046822	2.043074
244.750620	1242.844505	18.499866	-0.046735	2.037588
244.723189	1234.902103	18.504871	-0.046724	2.032081
244.783414	1226.923464	18.509875	-0.046731	2.026544
244.532855	1219.025074	18.514880	-0.046679	2.021015
244.542119	1211.100120	18.519885	-0.046676	2.015480
244.373437	1203.162207	18.524890	-0.046639	2.009901
244.411653	1195.229168	18.529895	-0.046641	2.004332
244.404477	1187.315766	18.534899	-0.046635	1.998757
244.539647	1179.361843	18.539904	-0.046655	1.993152
244.547643	1171.425046	18.544909	-0.046651	1.987530
244.259899	1163.544305	18.549914	-0.046593	1.981901
244.144961	1155.648412	18.554919	-0.046566	1.976264
244.144101	1147.696817	18.559923	-0.046561	1.970582
244.071773	1139.767476	18.564928	-0.046543	1.964892
243.814107	1131.916144	18.569933	-0.046490	1.959222
243.791594	1123.968210	18.574938	-0.046480	1.953491
243.867135	1115.984915	18.579943	-0.046489	1.947729
243.736973	1108.082011	18.584947	-0.046460	1.941985
243.492200	1100.192336	18.589952	-0.046410	1.936221
243.587550	1092.252969	18.594957	-0.046422	1.930441
243.560365	1084.322689	18.599962	-0.046412	1.924637
243.400106	1076.455921	18.604967	-0.046377	1.918847
243.284081	1068.541096	18.609971	-0.046351	1.913009
243.206419	1060.608598	18.614976	-0.046331	1.907144
242.967872	1052.736659	18.619981	-0.046282	1.901288
243.234538	1044.773369	18.624986	-0.046326	1.895403
243.390822	1036.842506	18.629991	-0.046350	1.889511
243.157565	1028.970767	18.634995	-0.046302	1.883601
242.805043	1021.109610	18.640000	-0.046231	1.877667
243.107938	1013.154716	18.645005	-0.046283	1.871718
242.918147	1005.237550	18.650010	-0.046242	1.865722
242.880759	997.348022	18.655015	-0.046230	1.859745
242.747379	989.451528	18.660019	-0.046200	1.853733
242.737280	981.527300	18.665024	-0.046193	1.847694
242.731573	973.643157	18.670029	-0.046187	1.841666
242.354927	965.788257	18.675034	-0.046112	1.835598
242.407321	957.853827	18.680039	-0.046117	1.829498
242.462411	949.934858	18.685043	-0.046122	1.823391
242.279293	942.071971	18.690048	-0.046083	1.817278
242.264593	934.167593	18.695053	-0.046075	1.811132
242.294728	926.237938	18.700058	-0.046076	1.804951
242.146502	918.391218	18.705063	-0.046043	1.798793
242.131224	910.457226	18.710067	-0.046035	1.792560
242.142663	902.509878	18.715072	-0.046032	1.786299
241.917829	894.679409	18.720077	-0.045986	1.780079
241.661670	886.809079	18.725082	-0.045933	1.773801
241.798084	878.881483	18.730087	-0.045953	1.767505
241.738351	871.006462	18.735091	-0.045937	1.761203
241.524666	863.156636	18.740096	-0.045892	1.754880
241.642577	855.238780	18.745101	-0.045909	1.748520
241.484155	847.363446	18.750106	-0.045875	1.742137
241.157202	839.539800	18.755111	-0.045809	1.735751
241.227957	831.621636	18.760115	-0.045817	1.729315
241.226636	823.726781	18.765120	-0.045812	1.722865
241.271568	815.858354	18.770125	-0.045815	1.716418
240.898550	807.999946	18.775130	-0.045741	1.709901
240.977726	800.093066	18.780135	-0.045750	1.703378
241.015055	792.218993	18.785139	-0.045752	1.696851
240.760777	784.357721	18.790144	-0.045700	1.690272
240.792544	776.485590	18.795149	-0.045701	1.683695
240.682789	768.635516	18.800154	-0.045675	1.677093
240.642810	760.745445	18.805159	-0.045663	1.670440
240.510122	752.890625	18.810163	-0.045633	1.663777
240.690428	744.997645	18.815168	-0.045662	1.657098
240.725706	737.125320	18.820173	-0.045663	1.650389
240.255572	729.333699	18.825178	-0.045571	1.643654
240.150059	721.499476	18.830183	-0.045546	1.636904
240.177191	713.559347	18.835187	-0.045546	1.630052
239.854403	705.728349	18.840192	-0.045481	1.623218
239.979304	697.856847	18.845197	-0.045499	1.616382
239.993476	689.974356	18.850202	-0.045497	1.609492
239.843210	682.149058	18.855207	-0.045464	1.602600
239.948604	674.296693	18.860211	-0.045479	1.595690
239.627174	666.467093	18.865216	-0.045414	1.588709
239.766270	658.596677	18.870221	-0.045435	1.581727
239.468546	650.805184	18.875226	-0.045374	1.574721
239.489640	642.936286	18.880231	-0.045373	1.567661
239.676403	635.069589	18.885235	-0.045403	1.560596
239.547279	627.259554	18.890240	-0.045374	1.553503
239.475229	619.408063	18.895245	-0.045356	1.546348
239.124620	611.629018	18.900250	-0.045285	1.539185
239.076948	603.788346	18.905255	-0.045272	1.531976
238.989302	595.954077	18.910259	-0.045250	1.524734
238.918064	588.139931	18.915264	-0.045232	1.517478
238.939274	580.297619	18.920269	-0.045231	1.510175
238.763605	572.477146	18.925274	-0.045193	1.502827
238.841519	564.654313	18.930279	-0.045203	1.495480
238.692152	556.849226	18.935283	-0.045170	1.488077
238.466993	549.059235	18.940288	-0.045123	1.480641
238.456774	541.244165	18.945293	-0.045116	1.473176
238.565794	533.358873	18.950298	-0.045132	1.465625
238.442700	525.584840	18.955303	-0.045104	1.458105
238.192598	517.802955	18.960307	-0.045052	1.450519
238.117176	510.009130	18.965312	-0.045033	1.442908
238.139324	502.220478	18.970317	-0.045032	1.435279
237.869141	494.427297	18.975322	-0.044977	1.427556
238.017992	486.621788	18.980327	-0.045000	1.419848
237.870948	478.849129	18.985331	-0.044968	1.412082
237.698000	471.082089	18.990336	-0.044930	1.404274
237.485066	463.339626	18.995341	-0.044886	1.396440
237.406753	455.533603	19.000346	-0.044866	1.388520
237.250540	447.775704	19.005351	-0.044832	1.380591
237.119682	440.019498	19.010355	-0.044803	1.372622
237.060153	432.228241	19.015360	-0.044787	1.364582
237.072508	424.475670	19.020365	-0.044784	1.356548
236.804667	416.732037	19.025370	-0.044730	1.348426
236.854497	408.961100	19.030375	-0.044734	1.340281
236.890791	401.195509	19.035379	-0.044736	1.332091
236.655414	393.472914	19.040384	-0.044687	1.323847
236.612077	385.741311	19.045389	-0.044674	1.315576
236.531216	377.861993	19.050394	-0.044654	1.307086
236.405444	370.164600	19.055399	-0.044626	1.298730
236.303380	362.445089	19.060403	-0.044602	1.290300
236.052689	354.749100	19.065408	-0.044550	1.281814
236.170891	347.024858	19.070413	-0.044567	1.273308
236.036340	339.313121	19.075418	-0.044537	1.264711
236.009861	331.615293	19.080423	-0.044527	1.256091
236.015511	323.899565	19.085427	-0.044524	1.247398
235.803752	316.240566	19.090432	-0.044479	1.238667
235.760583	308.543305	19.095437	-0.044466	1.229862
235.400376	300.894271	19.100442	-0.044394	1.220987
235.660579	293.168366	19.105447	-0.044438	1.212080
235.386312	285.531488	19.110451	-0.044382	1.203106
235.414309	277.853272	19.115456	-0.044382	1.194076
235.456933	270.172608	19.120461	-0.044385	1.184976
235.019870	262.588076	19.125466	-0.044299	1.175824
234.930464	254.942285	19.130471	-0.044278	1.166598
234.959137	247.303084	19.135475	-0.044278	1.157330
234.809816	239.642163	19.140480	-0.044246	1.147923
234.712047	232.020273	19.145485	-0.044222	1.138498
234.721059	224.384556	19.150490	-0.044219	1.129000
234.587432	216.798017	19.155495	-0.044190	1.119453
234.493605	209.202629	19.160499	-0.044167	1.109820
234.349620	201.618870	19.165504	-0.044136	1.100107
234.374944	194.030843	19.170509	-0.044136	1.090340
234.035198	186.501588	19.175514	-0.044068	1.080479
233.934909	178.941133	19.180519	-0.044044	1.070540
233.882849	171.373641	19.185523	-0.044030	1.060510
233.849525	163.819972	19.190528	-0.044019	1.050407
233.696500	156.311811	19.195533	-0.043985	1.040239
233.514549	148.804053	19.200538	-0.043947	1.029965
233.506832	141.284894	19.205543	-0.043940	1.019613
233.204426	133.828297	19.210547	-0.043879	1.009170
233.220147	126.326555	19.215552	-0.043878	0.998633
233.145935	118.830786	19.220557	-0.043859	0.987970
232.881537	111.390621	19.225562	-0.043805	0.977222
232.569017	103.979507	19.230567	-0.043742	0.966385
232.474345	96.558164	19.235571	-0.043720	0.955466
232.240372	89.153081	19.240576	-0.043671	0.944409
232.188152	81.751374	19.245581	-0.043657	0.933273
232.084278	74.361699	19.250586	-0.043633	0.922008
231.931109	67.014342	19.255591	-0.043600	0.910655
231.615808	59.925945	19.260595	-0.043537	0.899521