Tue Mar 23 11:10:51 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.167939	0.082948	0.000000	0.000073	0.722691

0.159379	0.088639	0.005005	0.000075	0.722699
0.013831	0.109136	0.010010	0.000102	0.722689
0.163787	0.084263	0.015014	0.000074	0.722693
0.252693	0.069821	0.020019	0.000057	0.722695
0.179000	0.079395	0.025024	0.000071	0.722689
0.069892	0.073409	0.030029	0.000091	0.722639
0.037711	-0.060134	0.035034	0.000097	0.722366
0.147792	-0.078506	0.040038	0.000077	0.722368
0.248511	-0.095013	0.045043	0.000058	0.722371
0.219857	-0.093097	0.050048	0.000063	0.722365
0.350386	-0.112169	0.055053	0.000039	0.722373
0.152569	-0.081251	0.060058	0.000075	0.722365
0.225711	-0.091974	0.065062	0.000062	0.722370
0.286526	-0.102688	0.070067	0.000050	0.722370
0.236164	-0.095477	0.075072	0.000060	0.722367
0.388106	-0.118122	0.080077	0.000031	0.722376
0.388545	-0.121784	0.085082	0.000031	0.722369
0.119624	-0.085559	0.090086	0.000081	0.722346
0.300165	-0.254374	0.095091	0.000047	0.722078
0.316892	-0.260338	0.100096	0.000044	0.722072
0.194548	-0.232963	0.105101	0.000067	0.722083
0.103318	-0.221138	0.110106	0.000084	0.722075
0.131924	-0.225800	0.115110	0.000078	0.722076
0.267864	-0.248300	0.120115	0.000053	0.722079
0.234237	-0.362577	0.125120	0.000059	0.721843
0.121310	-0.388896	0.130125	0.000080	0.721752
0.066323	-0.383243	0.135130	0.000090	0.721744
0.270878	-0.418158	0.140134	0.000052	0.721747
0.174895	-0.399647	0.145139	0.000070	0.721750
0.198275	-0.516637	0.150144	0.000066	0.721529
0.311992	-0.581896	0.155149	0.000044	0.721440
0.369369	-0.593745	0.160154	0.000034	0.721437
0.319500	-0.584913	0.165158	0.000043	0.721437
0.170420	-0.659327	0.170163	0.000070	0.721239
0.230665	-0.732622	0.175168	0.000059	0.721116
0.013142	-0.689935	0.180173	0.000100	0.721124
-0.112431	-0.668814	0.185178	0.000123	0.721122
-0.288235	-0.739574	0.190182	0.000156	0.720921
-0.286911	-0.758574	0.195187	0.000155	0.720884
-0.206428	-0.778422	0.200192	0.000140	0.720873
0.091238	-0.862752	0.205197	0.000085	0.720812
-0.255034	-0.939466	0.210202	0.000149	0.720540
-0.007478	-0.981924	0.215206	0.000103	0.720543
0.210427	-1.024691	0.220211	0.000062	0.720535
0.182446	-1.177872	0.225216	0.000068	0.720224
0.150708	-1.168662	0.230221	0.000073	0.720231
0.040666	-1.179899	0.235226	0.000094	0.720171
-0.103519	-1.289499	0.240230	0.000121	0.719904
-0.481352	-1.223459	0.245235	0.000191	0.719902
-0.649241	-1.234399	0.250240	0.000222	0.719822
-0.458899	-1.377014	0.255245	0.000187	0.719608
-0.661573	-1.346792	0.260250	0.000224	0.719596
-0.862779	-1.373867	0.265254	0.000262	0.719472
-0.877384	-1.470915	0.270259	0.000264	0.719276
-0.591809	-1.526084	0.275264	0.000211	0.719268
-0.383906	-1.658572	0.280269	0.000172	0.719079
-0.235652	-1.746601	0.285274	0.000145	0.718958
-0.365113	-1.759030	0.290278	0.000169	0.718888
-0.482126	-1.860297	0.295283	0.000190	0.718647
-0.410500	-1.878079	0.300288	0.000177	0.718637
-0.337452	-2.009986	0.305293	0.000163	0.718403
-0.478815	-2.009795	0.310298	0.000190	0.718354
-0.560763	-2.096514	0.315302	0.000205	0.718154
-0.495173	-2.174880	0.320307	0.000193	0.718022
-0.871235	-2.173360	0.325312	0.000263	0.717893
-1.510893	-2.153669	0.330317	0.000382	0.717707
-1.584246	-2.142824	0.335322	0.000395	0.717703
-2.486999	-2.137777	0.340326	0.000563	0.717395
-3.193115	-2.016218	0.345331	0.000694	0.717387
-3.523433	-1.962728	0.350336	0.000756	0.717376
-3.564141	-2.092817	0.355341	0.000763	0.717105
-3.775700	-2.065404	0.360346	0.000803	0.717085
-4.152401	-1.999074	0.365350	0.000873	0.717083
-3.991980	-2.141978	0.370355	0.000843	0.716857
-5.397756	-1.945366	0.375360	0.001104	0.716751
-4.731327	-2.058974	0.380365	0.000980	0.716761
-4.581714	-2.100292	0.385370	0.000952	0.716732
-6.008564	-1.988707	0.390374	0.001218	0.716450
-5.683722	-2.043376	0.395379	0.001157	0.716457
-5.909045	-2.009204	0.400384	0.001199	0.716445
-5.833947	-2.020419	0.405389	0.001185	0.716450
-6.358044	-2.060490	0.410394	0.001283	0.716186
-6.778322	-2.012273	0.415398	0.001361	0.716133
-6.480986	-2.063227	0.420403	0.001305	0.716137
-6.567456	-2.050197	0.425408	0.001321	0.716133
-6.793453	-2.048041	0.430413	0.001363	0.716057
-7.398085	-2.027782	0.435418	0.001476	0.715884
-7.334326	-2.036743	0.440422	0.001464	0.715889
-7.664881	-1.976578	0.445427	0.001525	0.715892
-7.394954	-2.028323	0.450432	0.001475	0.715885
-7.409491	-2.120698	0.455437	0.001478	0.715697
-8.579742	-1.988276	0.460442	0.001695	0.715546
-8.175950	-2.059455	0.465446	0.001620	0.715548
-8.353539	-2.025353	0.470451	0.001653	0.715553
-8.935351	-1.926300	0.475456	0.001761	0.715544
-8.018936	-2.130218	0.480461	0.001591	0.715463
-9.003492	-2.069197	0.485466	0.001774	0.715237
-9.477255	-1.986081	0.490470	0.001862	0.715234
-9.529860	-1.973375	0.495475	0.001872	0.715241
-9.109662	-2.052394	0.500480	0.001793	0.715233
-9.140861	-2.041141	0.505485	0.001799	0.715244
-9.710250	-2.021819	0.510490	0.001905	0.715082
-10.455507	-1.975083	0.515494	0.002044	0.714911
-9.862682	-2.077537	0.520499	0.001933	0.714918
-10.496525	-1.970583	0.525504	0.002051	0.714906
-10.492604	-1.966925	0.530509	0.002050	0.714915
-9.962852	-2.063807	0.535514	0.001952	0.714910
-10.411094	-2.020066	0.540518	0.002035	0.714838
-11.199424	-1.994865	0.545523	0.002182	0.714610
-10.962997	-2.040522	0.550528	0.002138	0.714603
-11.317768	-1.971286	0.555533	0.002203	0.714615
-11.189604	-1.997855	0.560538	0.002180	0.714608
-11.172157	-1.998220	0.565542	0.002176	0.714613
-11.011920	-2.024528	0.570547	0.002146	0.714618
-11.660180	-2.034256	0.575552	0.002267	0.714370
-12.419703	-1.940261	0.580557	0.002408	0.714288
-11.830882	-2.050770	0.585562	0.002299	0.714277
-12.114852	-2.000077	0.590566	0.002351	0.714277
-12.263077	-1.970540	0.595571	0.002379	0.714283
-12.082291	-2.007150	0.600576	0.002345	0.714275
-12.060777	-2.004626	0.605581	0.002341	0.714288
-12.452158	-2.063070	0.610586	0.002414	0.714033
-13.282285	-1.947917	0.615590	0.002568	0.713968
-12.837070	-2.024560	0.620595	0.002485	0.713974
-13.137106	-1.975834	0.625600	0.002541	0.713965
-13.294906	-1.943611	0.630605	0.002570	0.713973
-12.855415	-2.024221	0.635610	0.002488	0.713968
-13.213984	-1.960475	0.640614	0.002555	0.713968
-13.290038	-2.049239	0.645619	0.002569	0.713765
-14.370751	-1.917336	0.650624	0.002770	0.713645
-13.806834	-2.012066	0.655629	0.002665	0.713656
-13.846506	-2.006969	0.660634	0.002672	0.713653
-14.126487	-1.958241	0.665638	0.002724	0.713650
-13.608342	-2.046348	0.670643	0.002628	0.713659
-14.055877	-1.971659	0.675648	0.002711	0.713649
-14.346662	-2.003291	0.680653	0.002765	0.713483
-14.903060	-1.967151	0.685658	0.002869	0.713358
-14.898418	-1.970379	0.690662	0.002868	0.713354
-15.078916	-1.932428	0.695667	0.002901	0.713365
-15.212496	-1.914838	0.700672	0.002926	0.713353
-14.748502	-1.993028	0.705677	0.002840	0.713362
-14.932178	-1.962905	0.710682	0.002874	0.713357
-15.391161	-1.881858	0.715686	0.002959	0.713356
-15.216653	-2.071080	0.720691	0.002927	0.713041
-15.786278	-1.979849	0.725696	0.003032	0.713021
-16.029402	-1.934625	0.730701	0.003078	0.713025
-15.711883	-1.994881	0.735706	0.003018	0.713018
-15.911359	-1.960413	0.740710	0.003055	0.713016
-15.668986	-1.998265	0.745715	0.003010	0.713027
-15.863756	-1.965968	0.750720	0.003046	0.713022
-16.297956	-2.026730	0.755725	0.003127	0.712747
-17.021606	-1.919065	0.760730	0.003262	0.712705
-17.126725	-1.899877	0.765734	0.003281	0.712706
-16.629210	-1.984634	0.770739	0.003189	0.712714
-16.977865	-1.927038	0.775744	0.003253	0.712705
-17.132373	-1.894818	0.780749	0.003282	0.712715
-16.944609	-1.929647	0.785754	0.003247	0.712712
-16.917561	-1.949443	0.790758	0.003242	0.712683
-17.710726	-1.952923	0.795763	0.003389	0.712394
-17.874270	-1.928026	0.800768	0.003420	0.712386
-18.103177	-1.885061	0.805773	0.003462	0.712391
-17.865699	-1.928981	0.810778	0.003418	0.712388
-18.173815	-1.876958	0.815782	0.003475	0.712382
-17.795421	-1.939911	0.820787	0.003405	0.712391
-17.800743	-1.943318	0.825792	0.003406	0.712383
-17.983953	-1.930704	0.830797	0.003440	0.712343
-18.502752	-1.965014	0.835802	0.003536	0.712091
-18.505458	-1.965480	0.840806	0.003537	0.712089
-18.959564	-1.880829	0.845811	0.003621	0.712096
-18.822793	-1.911546	0.850816	0.003596	0.712084
-18.647331	-1.938153	0.855821	0.003563	0.712093
-18.965934	-1.884064	0.860826	0.003622	0.712088
-18.542452	-1.960417	0.865830	0.003543	0.712087
-18.702686	-2.072844	0.870835	0.003573	0.711806
-19.741825	-1.912223	0.875840	0.003766	0.711757
-19.700874	-1.915692	0.880845	0.003758	0.711765
-19.497709	-1.954751	0.885850	0.003721	0.711759
-19.833877	-1.894399	0.890854	0.003783	0.711760
-19.869313	-1.884259	0.895859	0.003790	0.711768
-19.831992	-1.896669	0.900864	0.003783	0.711757
-19.758600	-1.993960	0.905869	0.003769	0.711589
-20.891843	-1.858460	0.910874	0.003980	0.711457
-20.733184	-1.887047	0.915878	0.003950	0.711456
-20.464279	-1.933399	0.920883	0.003900	0.711460
-20.440216	-1.942271	0.925888	0.003895	0.711451
-20.521895	-1.922915	0.930893	0.003910	0.711460
-20.841659	-1.869279	0.935898	0.003970	0.711454
-20.726194	-1.894122	0.940902	0.003948	0.711446
-21.185727	-1.963647	0.945907	0.004034	0.711144
-21.664984	-1.881788	0.950912	0.004123	0.711137
-21.616985	-1.888314	0.955917	0.004114	0.711141
-21.373571	-1.933684	0.960922	0.004069	0.711137
-21.841690	-1.851737	0.965926	0.004156	0.711134
-21.577749	-1.894430	0.970931	0.004106	0.711143
-21.657332	-1.886241	0.975936	0.004121	0.711131
-21.718683	-1.931499	0.980941	0.004132	0.711019
-22.366710	-1.891685	0.985946	0.004253	0.710869
-21.879121	-1.978214	0.990950	0.004162	0.710869
-22.324050	-1.895785	0.995955	0.004245	0.710876
-22.632566	-1.845711	1.000960	0.004302	0.710866
-22.149875	-1.927810	1.005965	0.004212	0.710874
-22.331501	-1.899601	1.010970	0.004246	0.710866
-22.932449	-1.886092	1.015974	0.004358	0.710679
-23.605800	-1.838913	1.020979	0.004483	0.710534
-23.058075	-1.940417	1.025984	0.004381	0.710527
-23.347051	-1.884601	1.030989	0.004435	0.710535
-23.640418	-1.834527	1.035994	0.004489	0.710531
-23.552525	-1.852266	1.040998	0.004473	0.710527
-23.002817	-1.945294	1.046003	0.004370	0.710537
-23.372195	-1.885623	1.051008	0.004439	0.710525
-23.791526	-1.963115	1.056013	0.004517	0.710221
-23.736517	-1.974916	1.061018	0.004507	0.710217
-24.451443	-1.849377	1.066022	0.004640	0.710214
-23.820684	-1.957944	1.071027	0.004522	0.710221
-23.941168	-1.941639	1.076032	0.004545	0.710211
-24.212932	-1.889517	1.081037	0.004595	0.710219
-24.094094	-1.961924	1.086042	0.004573	0.710117
-25.081791	-1.898910	1.091046	0.004757	0.709891
-24.636514	-1.973652	1.096051	0.004674	0.709900
-25.531101	-1.819610	1.101056	0.004840	0.709890
-25.294064	-1.859004	1.106061	0.004796	0.709896
-24.736555	-1.960379	1.111066	0.004692	0.709892
-25.238024	-1.872128	1.116070	0.004785	0.709890
-25.130320	-1.897844	1.121075	0.004765	0.709877
-25.627036	-1.952271	1.126080	0.004858	0.709591
-25.639223	-1.946285	1.131085	0.004860	0.709599
-26.144571	-1.856716	1.136090	0.004954	0.709598
-25.786972	-1.922315	1.141094	0.004887	0.709595
-25.448451	-1.978897	1.146099	0.004824	0.709602
-26.028019	-1.882853	1.151104	0.004932	0.709588
-25.726072	-1.992560	1.156109	0.004875	0.709476
-26.621281	-1.939362	1.161114	0.005042	0.709264
-26.642493	-1.936838	1.166118	0.005046	0.709261
-26.740137	-1.915392	1.171123	0.005064	0.709270
-26.970322	-1.880740	1.176128	0.005107	0.709257
-26.781057	-1.909092	1.181133	0.005071	0.709268
-26.910442	-1.888931	1.186138	0.005095	0.709262
-26.807197	-1.947885	1.191142	0.005076	0.709181
-27.157572	-1.994800	1.196147	0.005141	0.708962
-27.689670	-1.906579	1.201152	0.005240	0.708949
-28.107899	-1.828166	1.206157	0.005318	0.708957
-27.468266	-1.944256	1.211162	0.005199	0.708953
-27.663014	-1.909600	1.216166	0.005235	0.708953
-27.811903	-1.881129	1.221171	0.005263	0.708957
-27.843217	-1.897733	1.226176	0.005268	0.708913
-28.411786	-1.932368	1.231181	0.005374	0.708641
-28.538878	-1.910314	1.236186	0.005398	0.708640
-28.885939	-1.850698	1.241190	0.005462	0.708636
-28.084144	-1.989414	1.246195	0.005313	0.708644
-28.623884	-1.898035	1.251200	0.005413	0.708635
-28.796214	-1.863946	1.256205	0.005445	0.708642
-28.474895	-1.925419	1.261210	0.005385	0.708633
-29.170119	-1.943501	1.266214	0.005515	0.708349
-29.500264	-1.882303	1.271219	0.005576	0.708354
-29.642829	-1.862357	1.276224	0.005603	0.708343
-29.402799	-1.901790	1.281229	0.005558	0.708350
-29.544161	-1.876608	1.286234	0.005584	0.708350
-29.809081	-1.832796	1.291238	0.005633	0.708344
-29.136325	-1.946497	1.296243	0.005508	0.708356
-29.845282	-1.960982	1.301248	0.005640	0.708074
-30.635271	-1.851154	1.306253	0.005787	0.708012
-30.344246	-1.905398	1.311258	0.005733	0.708008
-30.057695	-1.957756	1.316262	0.005679	0.708005
-30.531889	-1.869136	1.321267	0.005767	0.708014
-30.460581	-1.886716	1.326272	0.005754	0.708004
-30.043784	-1.956018	1.331277	0.005676	0.708014
-30.500902	-1.995272	1.336282	0.005761	0.707772
-31.742029	-1.812345	1.341286	0.005992	0.707696
-31.084254	-1.927434	1.346291	0.005870	0.707700
-31.050419	-1.935729	1.351296	0.005863	0.707696
-31.433505	-1.866029	1.356301	0.005935	0.707699
-31.091382	-1.928251	1.361306	0.005871	0.707696
-31.194308	-1.912329	1.366310	0.005890	0.707692
-31.168933	-2.026815	1.371315	0.005885	0.707471
-32.326982	-1.869209	1.376320	0.006101	0.707374
-32.239270	-1.883021	1.381325	0.006084	0.707377
-32.031690	-1.919673	1.386330	0.006045	0.707378
-32.295535	-1.876782	1.391334	0.006094	0.707370
-31.975287	-1.929858	1.396339	0.006035	0.707378
-32.147481	-1.902990	1.401344	0.006067	0.707371
-32.436194	-1.945589	1.406349	0.006120	0.707182
-32.910115	-1.911667	1.411354	0.006209	0.707081
-32.912389	-1.915001	1.416358	0.006209	0.707073
-32.915640	-1.908367	1.421363	0.006209	0.707086
-33.207381	-1.859648	1.426368	0.006264	0.707079
-32.669847	-1.953121	1.431373	0.006163	0.707084
-32.645154	-1.958891	1.436378	0.006159	0.707082
-33.647160	-1.925340	1.441382	0.006345	0.706791
-33.931112	-1.891292	1.446387	0.006398	0.706757
-33.873276	-1.906736	1.451392	0.006387	0.706747
-33.965466	-1.887595	1.456397	0.006404	0.706753
-33.768198	-1.923382	1.461402	0.006367	0.706752
-33.895886	-1.902305	1.466406	0.006391	0.706749
-33.753729	-1.922327	1.471411	0.006365	0.706759
-34.229861	-1.943670	1.476416	0.006453	0.706546
-35.126917	-1.833313	1.481421	0.006620	0.706447
-34.662933	-1.916713	1.486426	0.006534	0.706446
-34.698616	-1.913741	1.491430	0.006540	0.706439
-34.636297	-1.918837	1.496435	0.006528	0.706451
-34.697569	-1.913867	1.501440	0.006540	0.706439
-34.885128	-1.876759	1.506445	0.006575	0.706447
-34.734454	-1.987327	1.511450	0.006546	0.706279
-35.917090	-1.852985	1.516454	0.006766	0.706125
-35.630897	-1.899422	1.521459	0.006713	0.706135
-35.816000	-1.870670	1.526464	0.006747	0.706126
-35.675233	-1.893904	1.531469	0.006721	0.706130
-35.458503	-1.932268	1.536474	0.006681	0.706131
-35.935747	-1.851877	1.541478	0.006769	0.706122
-35.508727	-1.972621	1.546483	0.006690	0.706032
-36.213093	-1.932917	1.551488	0.006821	0.705860
-36.479373	-1.883992	1.556493	0.006870	0.705863
-36.597453	-1.863770	1.561498	0.006892	0.705861
-36.318433	-1.916380	1.566502	0.006840	0.705856
-36.271106	-1.919004	1.571507	0.006831	0.705868
-36.508146	-1.882080	1.576512	0.006875	0.705857
-36.620590	-1.976086	1.581517	0.006896	0.705628
-37.276750	-1.909557	1.586522	0.007018	0.705526
-37.583441	-1.858974	1.591526	0.007075	0.705518
-36.933903	-1.969945	1.596531	0.006954	0.705528
-37.309937	-1.908205	1.601536	0.007024	0.705518
-37.460628	-1.879300	1.606541	0.007052	0.705522
-37.260056	-1.914050	1.611546	0.007015	0.705524
-37.669487	-1.980298	1.616550	0.007091	0.705244
-38.020885	-1.933333	1.621555	0.007156	0.705213
-38.423312	-1.864715	1.626560	0.007231	0.705207
-37.991752	-1.940598	1.631565	0.007151	0.705209
-37.902056	-1.957214	1.636570	0.007134	0.705208
-38.397654	-1.871679	1.641574	0.007226	0.705202
-38.144531	-1.924129	1.646579	0.007179	0.705188
-38.659312	-1.984661	1.651584	0.007275	0.704881
-38.832004	-1.951991	1.656589	0.007307	0.704885
-39.312100	-1.866271	1.661594	0.007396	0.704886
-39.138359	-1.900773	1.666598	0.007364	0.704879
-38.859653	-1.945036	1.671603	0.007312	0.704890
-39.275943	-1.874137	1.676608	0.007389	0.704883
-39.017732	-1.944226	1.681613	0.007341	0.704835
-39.650937	-1.953212	1.686618	0.007459	0.704590
-40.046266	-1.885736	1.691622	0.007532	0.704584
-40.116850	-1.868904	1.696627	0.007545	0.704593
-39.625576	-1.962212	1.701632	0.007454	0.704581
-39.941624	-1.902827	1.706637	0.007512	0.704587
-40.082442	-1.877581	1.711642	0.007539	0.704588
-39.824097	-1.946716	1.716646	0.007490	0.704542
-40.278915	-2.005751	1.721651	0.007575	0.704259
-40.816360	-1.913366	1.726656	0.007675	0.704253
-40.976328	-1.882809	1.731661	0.007705	0.704257
-40.313598	-2.000756	1.736666	0.007581	0.704257
-40.730039	-1.928779	1.741670	0.007659	0.704253
-40.985369	-1.878864	1.746675	0.007706	0.704262
-40.833316	-1.964142	1.751680	0.007678	0.704145
-41.663910	-1.914640	1.756685	0.007832	0.703946
-41.631424	-1.919241	1.761690	0.007826	0.703949
-41.884429	-1.877632	1.766694	0.007873	0.703942
-41.620354	-1.919994	1.771699	0.007824	0.703952
-41.572134	-1.931809	1.776704	0.007815	0.703945
-41.677118	-1.910667	1.781709	0.007834	0.703950
-41.658987	-1.965317	1.786714	0.007831	0.703847
-42.938025	-1.843757	1.791718	0.008069	0.703632
-42.584622	-1.904442	1.796723	0.008003	0.703637
-42.541788	-1.914562	1.801728	0.007995	0.703632
-42.635148	-1.897658	1.806733	0.008012	0.703633
-42.580794	-1.904765	1.811738	0.008002	0.703638
-42.885116	-1.852614	1.816742	0.008059	0.703634
-42.460125	-1.930546	1.821747	0.007979	0.703630
-43.162243	-1.951215	1.826752	0.008110	0.703336
-43.826901	-1.833051	1.831757	0.008234	0.703335
-43.548924	-1.879559	1.836762	0.008182	0.703342
-43.201210	-1.946847	1.841766	0.008117	0.703331
-43.586888	-1.870026	1.846771	0.008189	0.703348
-43.781973	-1.841173	1.851776	0.008225	0.703336
-43.388985	-1.910077	1.856781	0.008152	0.703338
-43.707401	-1.983511	1.861786	0.008211	0.703075
-44.692227	-1.846360	1.866790	0.008394	0.702998
-44.274247	-1.916747	1.871795	0.008316	0.703007
-44.027668	-1.965387	1.876800	0.008270	0.702997
-44.636609	-1.854950	1.881805	0.008383	0.703001
-44.090170	-1.949434	1.886810	0.008282	0.703007
-43.997873	-1.975400	1.891814	0.008264	0.702988
-44.876332	-1.965145	1.896819	0.008428	0.702693
-45.074586	-1.932708	1.901824	0.008465	0.702687
-45.514349	-1.852621	1.906829	0.008546	0.702691
-45.163029	-1.912596	1.911834	0.008481	0.702696
-45.422463	-1.871723	1.916838	0.008529	0.702685
-45.211470	-1.906488	1.921843	0.008490	0.702691
-45.380727	-1.880262	1.926848	0.008521	0.702684
-45.859684	-1.930890	1.931853	0.008610	0.702409
-46.020073	-1.923495	1.936858	0.008640	0.702366
-46.210492	-1.892413	1.941862	0.008675	0.702360
-46.179540	-1.893772	1.946867	0.008670	0.702369
-46.291610	-1.876696	1.951872	0.008690	0.702363
-45.871177	-1.949188	1.956877	0.008612	0.702368
-45.857556	-1.949348	1.961882	0.008609	0.702373
-46.935901	-1.892515	1.966886	0.008810	0.702100
-46.851827	-1.919317	1.971891	0.008794	0.702076
-46.802026	-1.932641	1.976896	0.008785	0.702067
-47.148408	-1.869510	1.981901	0.008849	0.702070
-47.085362	-1.877827	1.986906	0.008838	0.702076
-47.076245	-1.885055	1.991910	0.008836	0.702065
-46.910840	-1.909846	1.996915	0.008805	0.702075
-47.670864	-1.915527	2.001920	0.008946	0.701789

-47.974209	-1.886406	2.011917	0.009003	0.701739
-47.917357	-1.895170	2.021914	0.008992	0.701742
-47.985847	-1.883093	2.031910	0.009004	0.701742
-47.760066	-1.924135	2.041907	0.008962	0.701741
-47.910114	-1.896438	2.051904	0.008990	0.701743
-47.658672	-1.942982	2.061901	0.008943	0.701740
-47.759881	-1.923296	2.071898	0.008962	0.701744
-47.925170	-1.895351	2.081894	0.008992	0.701741
-47.953775	-1.890887	2.091891	0.008997	0.701740
-47.759654	-1.924896	2.101888	0.008961	0.701742
-47.918266	-1.895555	2.111885	0.008990	0.701744
-47.392726	-1.916213	2.121882	0.008892	0.701892
-46.805668	-1.931598	2.131878	0.008783	0.702073
-46.850890	-1.923399	2.141875	0.008791	0.702074
-47.003255	-1.896177	2.151872	0.008819	0.702074
-46.918374	-1.910477	2.161869	0.008803	0.702076
-46.780363	-1.936838	2.171866	0.008777	0.702073
-46.533529	-1.883159	2.181862	0.008731	0.702271
-46.226972	-1.888793	2.191859	0.008674	0.702371
-46.223939	-1.890666	2.201856	0.008673	0.702368
-46.244762	-1.887435	2.211853	0.008677	0.702368
-45.574692	-1.907773	2.221850	0.008552	0.702568
-45.310572	-1.892789	2.231846	0.008503	0.702694
-45.053561	-1.939707	2.241843	0.008455	0.702692
-45.481537	-1.863082	2.251840	0.008534	0.702693
-44.870970	-1.867618	2.261837	0.008420	0.702904
-44.538809	-1.877922	2.271834	0.008358	0.703004
-44.336990	-1.913492	2.281830	0.008321	0.703005
-44.319112	-1.917315	2.291827	0.008317	0.703004
-43.761495	-1.855207	2.301824	0.008213	0.703330
-43.475434	-1.903587	2.311821	0.008160	0.703336
-43.157668	-1.958625	2.321818	0.008100	0.703340
-43.439830	-1.879163	2.331814	0.008153	0.703399
-42.484406	-1.932513	2.341811	0.007974	0.703635
-42.815315	-1.875092	2.351808	0.008036	0.703633
-42.459994	-1.937790	2.361805	0.007970	0.703634
-42.229429	-1.886130	2.371802	0.007926	0.703822
-41.709186	-1.913854	2.381798	0.007829	0.703953
-41.998479	-1.862730	2.391795	0.007883	0.703953
-41.771828	-1.881689	2.401792	0.007841	0.703996
-40.903236	-1.905577	2.411789	0.007679	0.704261
-41.046861	-1.879528	2.421786	0.007705	0.704262
-40.830303	-1.917178	2.431782	0.007665	0.704264
-40.259090	-1.908860	2.441779	0.007558	0.704487
-40.100891	-1.885629	2.451776	0.007529	0.704591
-39.873957	-1.925244	2.461773	0.007486	0.704593
-39.878422	-1.923496	2.471770	0.007487	0.704595
-39.186129	-1.900320	2.481766	0.007358	0.704891
-39.167545	-1.904581	2.491763	0.007354	0.704889
-39.014801	-1.932095	2.501760	0.007326	0.704889
-38.840522	-1.897694	2.511757	0.007293	0.705021
-38.130503	-1.928812	2.521754	0.007161	0.705214
-38.068613	-1.941451	2.531750	0.007149	0.705211
-38.197398	-1.917932	2.541747	0.007173	0.705212
-37.652895	-1.883494	2.551744	0.007071	0.705477
-37.349677	-1.913562	2.561741	0.007014	0.705526
-37.276112	-1.928748	2.571738	0.007001	0.705522
-37.319808	-1.852638	2.581734	0.007008	0.705660
-36.349359	-1.926619	2.591731	0.006828	0.705860
-36.490866	-1.901532	2.601728	0.006854	0.705860
-36.553347	-1.892161	2.611725	0.006865	0.705856
-35.803924	-1.903519	2.621722	0.006726	0.706103
-35.665387	-1.915637	2.631718	0.006700	0.706128
-35.675525	-1.915595	2.641715	0.006701	0.706125
-35.395357	-1.885018	2.651712	0.006649	0.706287
-34.887599	-1.900076	2.661709	0.006554	0.706439
-35.003235	-1.877617	2.671706	0.006576	0.706443
-34.649343	-1.910457	2.681702	0.006509	0.706505
-33.936430	-1.914951	2.691699	0.006377	0.706751
-33.951078	-1.912746	2.701696	0.006379	0.706751
-33.923293	-1.918765	2.711693	0.006374	0.706749
-33.459687	-1.886992	2.721690	0.006287	0.706979
-33.022062	-1.913675	2.731686	0.006206	0.707082
-33.150728	-1.892357	2.741683	0.006229	0.707080
-33.064978	-1.868232	2.751680	0.006213	0.707159
-32.096631	-1.933891	2.761677	0.006033	0.707374
-32.300259	-1.896217	2.771674	0.006070	0.707377
-32.317868	-1.892979	2.781670	0.006074	0.707378
-31.549884	-1.882545	2.791667	0.005930	0.707674
-31.518053	-1.876432	2.801664	0.005924	0.707698
-31.400473	-1.896467	2.811661	0.005902	0.707700
-31.093789	-1.869486	2.821658	0.005845	0.707864
-30.553966	-1.891825	2.831654	0.005744	0.708012
-30.591274	-1.886128	2.841651	0.005751	0.708011
-30.211547	-1.949059	2.851648	0.005680	0.708021
-29.995871	-1.825709	2.861645	0.005640	0.708345
-29.406066	-1.927904	2.871642	0.005530	0.708352
-29.674224	-1.880953	2.881638	0.005579	0.708350
-29.297653	-1.859052	2.891635	0.005509	0.708529
-28.857192	-1.883774	2.901632	0.005427	0.708637
-28.792706	-1.895515	2.911629	0.005415	0.708637
-28.695663	-1.880799	2.921626	0.005397	0.708701
-27.980797	-1.881749	2.931622	0.005263	0.708955
-28.086746	-1.862652	2.941619	0.005283	0.708956
-27.819887	-1.910728	2.951616	0.005233	0.708955
-27.487193	-1.847433	2.961613	0.005171	0.709201
-26.876034	-1.924611	2.971610	0.005057	0.709265
-27.087300	-1.887646	2.981606	0.005096	0.709264
-27.023936	-1.848430	2.991603	0.005084	0.709365
-26.072493	-1.902537	3.001600	0.004907	0.709596
-26.168879	-1.887371	3.011597	0.004924	0.709593
-26.253339	-1.871478	3.021594	0.004940	0.709595
-25.680109	-1.847173	3.031590	0.004833	0.709848
-25.249885	-1.903019	3.041587	0.004753	0.709890
-25.231053	-1.906664	3.051584	0.004749	0.709890
-25.490973	-1.794673	3.061581	0.004797	0.710021
-24.230795	-1.921615	3.071578	0.004563	0.710217
-24.643612	-1.846748	3.081574	0.004639	0.710220
-24.512080	-1.864061	3.091571	0.004614	0.710233
-23.713899	-1.856518	3.101568	0.004466	0.710532
-23.667245	-1.865120	3.111565	0.004457	0.710532
-23.334283	-1.924187	3.121562	0.004395	0.710533
-23.330147	-1.835513	3.131558	0.004394	0.710712
-22.648975	-1.877108	3.141555	0.004267	0.710871
-22.750610	-1.859172	3.151552	0.004285	0.710871
-22.772926	-1.849968	3.161549	0.004289	0.710882
-22.010105	-1.856960	3.171546	0.004147	0.711140
-21.971378	-1.863836	3.181542	0.004140	0.711140
-21.815896	-1.892414	3.191539	0.004111	0.711139
-21.455485	-1.853429	3.201536	0.004043	0.711345
-20.999342	-1.879686	3.211533	0.003958	0.711455
-20.976123	-1.883329	3.221530	0.003954	0.711457
-20.909172	-1.876785	3.231526	0.003941	0.711494
-20.089731	-1.887863	3.241523	0.003788	0.711763
-20.203946	-1.869607	3.251520	0.003809	0.711759
-20.210386	-1.867143	3.261517	0.003810	0.711762
-19.445238	-1.891346	3.271514	0.003668	0.711986
-19.212868	-1.878936	3.281510	0.003624	0.712094
-18.989590	-1.918493	3.291507	0.003583	0.712095
-19.160242	-1.890380	3.301504	0.003614	0.712091
-18.590795	-1.848208	3.311501	0.003508	0.712377
-18.139274	-1.922974	3.321498	0.003424	0.712389
-18.401778	-1.877167	3.331494	0.003472	0.712387
-18.075344	-1.852608	3.341491	0.003411	0.712552
-17.435368	-1.887651	3.351488	0.003292	0.712710
-17.570532	-1.864255	3.361485	0.003317	0.712709
-17.574671	-1.837908	3.371482	0.003318	0.712760
-16.544427	-1.888120	3.381478	0.003126	0.713026
-16.385026	-1.917237	3.391475	0.003096	0.713025
-16.555993	-1.887111	3.401472	0.003128	0.713025
-16.312347	-1.854360	3.411469	0.003082	0.713177
-15.285724	-1.946222	3.421466	0.002891	0.713358
-15.531383	-1.900512	3.431462	0.002936	0.713362
-15.344493	-1.933505	3.441459	0.002901	0.713363
-15.147347	-1.876324	3.451456	0.002864	0.713547
-14.623214	-1.916975	3.461453	0.002767	0.713652
-14.922726	-1.862026	3.471450	0.002822	0.713656
-14.759137	-1.856051	3.481446	0.002791	0.713726
-13.930751	-1.880128	3.491443	0.002637	0.713972
-13.955803	-1.875327	3.501440	0.002642	0.713973
-13.739689	-1.914624	3.511437	0.002601	0.713972
-13.215456	-1.893167	3.521434	0.002503	0.714200
-13.148472	-1.863386	3.531430	0.002491	0.714283
-12.956283	-1.899011	3.541427	0.002455	0.714281
-13.117926	-1.822640	3.551424	0.002485	0.714376
-11.908155	-1.919719	3.561421	0.002259	0.714611
-12.069514	-1.889104	3.571418	0.002289	0.714616
-11.636680	-1.966570	3.581414	0.002208	0.714615
-11.427546	-1.922685	3.591411	0.002169	0.714777
-10.796147	-1.967576	3.601408	0.002051	0.714911
-11.094982	-1.914245	3.611405	0.002107	0.714912
-10.745442	-1.977385	3.621402	0.002042	0.714910
-10.519042	-1.929806	3.631398	0.001999	0.715085
-9.985360	-1.948555	3.641395	0.001900	0.715237
-10.200133	-1.910552	3.651392	0.001940	0.715237
-9.993771	-1.947283	3.661389	0.001901	0.715237
-9.441773	-1.911321	3.671386	0.001798	0.715504
-8.941035	-1.975106	3.681382	0.001705	0.715555
-9.034780	-1.961655	3.691379	0.001722	0.715548
-8.755408	-2.011586	3.701376	0.001670	0.715548
-8.046372	-1.976998	3.711373	0.001537	0.715868
-7.906240	-1.992391	3.721370	0.001511	0.715887
-7.729570	-2.023950	3.731366	0.001478	0.715887
-8.217625	-1.937000	3.741363	0.001569	0.715888
-7.326496	-1.981300	3.751360	0.001403	0.716115
-7.049411	-2.021553	3.761357	0.001351	0.716133
-7.057226	-2.018441	3.771354	0.001352	0.716137
-7.016518	-1.995888	3.781350	0.001344	0.716196
-6.165525	-2.017438	3.791347	0.001186	0.716454
-5.856899	-2.072339	3.801344	0.001128	0.716455
-6.360048	-1.982823	3.811341	0.001222	0.716455
-5.875864	-2.020336	3.821338	0.001131	0.716552
-4.898876	-2.087228	3.831334	0.000949	0.716764
-5.074131	-2.056504	3.841331	0.000982	0.716763
-5.131256	-2.047174	3.851328	0.000992	0.716762
-4.896924	-2.039218	3.861325	0.000948	0.716861
-4.206111	-2.046997	3.871322	0.000820	0.717089
-4.109402	-2.062338	3.881318	0.000801	0.717093
-4.275912	-2.034160	3.891315	0.000832	0.717091
-3.583264	-2.073631	3.901312	0.000703	0.717257
-3.351430	-2.050732	3.911309	0.000660	0.717384
-3.372796	-2.045875	3.921306	0.000664	0.717387
-3.468316	-2.028048	3.931302	0.000681	0.717389
-2.922406	-1.970402	3.941299	0.000579	0.717695
-2.349676	-2.066163	3.951296	0.000473	0.717708
-2.707811	-2.002953	3.961293	0.000539	0.717707
-2.154995	-2.014200	3.971290	0.000436	0.717880
-1.809945	-2.003533	3.981286	0.000371	0.718023
-1.934283	-1.982077	3.991283	0.000394	0.718022
-1.766765	-1.968892	4.001280	0.000363	0.718107
-2.074722	-1.786569	4.011277	0.000420	0.718359
-1.827664	-1.829786	4.021274	0.000374	0.718361
-1.273296	-1.826025	4.031270	0.000270	0.718564
-1.766072	-1.695109	4.041267	0.000362	0.718649
-1.154305	-1.743651	4.051264	0.000248	0.718769
-1.119214	-1.651561	4.061261	0.000241	0.718963
-1.019527	-1.640891	4.071258	0.000222	0.719020
-1.120643	-1.494603	4.081254	0.000241	0.719273
-0.876703	-1.504258	4.091251	0.000195	0.719340
-1.146955	-1.322803	4.101248	0.000245	0.719603
-0.857169	-1.306196	4.111245	0.000191	0.719738
-0.810811	-1.229142	4.121242	0.000182	0.719907
-0.471746	-1.164957	4.131238	0.000119	0.720153
-0.643556	-1.067934	4.141235	0.000151	0.720284
-0.391105	-0.981712	4.151232	0.000104	0.720542
-0.542448	-0.847171	4.161229	0.000131	0.720755
-0.351717	-0.789941	4.171226	0.000096	0.720934
-0.519992	-0.661900	4.181222	0.000127	0.721128
-0.930455	-0.444785	4.191219	0.000203	0.721411
-0.700966	-0.358917	4.201216	0.000160	0.721661
-0.580887	-0.241836	4.211213	0.000137	0.721934
-0.253034	-0.167976	4.221210	0.000076	0.722194
0.057280	-0.094764	4.231206	0.000018	0.722446
0.039488	0.048050	4.241203	0.000021	0.722721
0.000000	0.258490	4.251200	0.000028	0.723120

0.002094	0.887953	4.256205	0.000027	0.724355
0.098979	2.129575	4.261210	0.000008	0.726817
0.316397	3.947524	4.266214	-0.000034	0.730433
0.820179	6.274278	4.271219	-0.000129	0.735111
0.970300	9.162496	4.276224	-0.000159	0.740716
1.221176	12.528065	4.281229	-0.000208	0.747220
1.874384	16.265680	4.286234	-0.000332	0.754501
2.024225	20.500621	4.291238	-0.000363	0.762473
2.646160	25.060369	4.296243	-0.000482	0.771114
3.036704	30.018040	4.301248	-0.000558	0.780308
3.559136	35.311787	4.306253	-0.000658	0.790040
3.891363	40.946551	4.311258	-0.000724	0.800199
4.427574	46.854476	4.316262	-0.000828	0.810772
4.937054	53.050286	4.321267	-0.000927	0.821697
5.070635	59.580769	4.326272	-0.000956	0.832936
5.758597	66.234239	4.331277	-0.001089	0.844396
6.222169	73.153721	4.336282	-0.001180	0.856077
6.483712	80.303871	4.341286	-0.001233	0.867920
7.131946	87.584517	4.346291	-0.001359	0.879924
7.497236	95.073663	4.351296	-0.001431	0.892018
9.140061	102.513354	4.356301	-0.001742	0.904224
10.238555	110.213741	4.361306	-0.001952	0.916522
10.614127	118.153251	4.366310	-0.002027	0.928829
11.669866	126.105796	4.371315	-0.002229	0.941174
12.388605	134.221780	4.376320	-0.002368	0.953513
13.286057	142.400786	4.381325	-0.002541	0.965833
13.807399	150.730507	4.386330	-0.002643	0.978121
14.226465	159.143132	4.391334	-0.002727	0.990349
15.527036	167.462019	4.396339	-0.002975	1.002512
16.601375	175.854593	4.401344	-0.003180	1.014576
17.349714	184.352572	4.406349	-0.003325	1.026566
17.848091	192.934505	4.411354	-0.003424	1.038472
18.815060	201.458070	4.416358	-0.003609	1.050274
19.317715	210.095112	4.421363	-0.003709	1.061988
19.655433	218.782275	4.426368	-0.003777	1.073603
20.274520	227.407274	4.431373	-0.003898	1.085075
20.929685	236.044132	4.436378	-0.004026	1.096450
21.616374	244.674433	4.441382	-0.004160	1.107707
22.255468	253.327192	4.446387	-0.004284	1.118868
22.836348	261.966805	4.451392	-0.004398	1.129890
23.442726	270.619779	4.456397	-0.004517	1.140826
24.047306	279.283642	4.461402	-0.004635	1.151672
24.715421	287.897785	4.466406	-0.004765	1.162369
25.467352	296.502484	4.471411	-0.004911	1.172973
25.949183	305.120695	4.476416	-0.005006	1.183444
26.367092	313.764433	4.481421	-0.005090	1.193839
26.898420	322.351274	4.486426	-0.005195	1.204100
27.507758	330.927573	4.491430	-0.005314	1.214278
28.037438	339.503223	4.496435	-0.005418	1.224354
28.656699	348.063239	4.501440	-0.005539	1.234347
29.519412	356.547411	4.506445	-0.005705	1.244220
29.918958	365.110238	4.511450	-0.005785	1.254016
30.620929	373.590378	4.516454	-0.005922	1.263700
31.227266	382.112786	4.521459	-0.006040	1.273338
31.514313	390.633278	4.526464	-0.006099	1.282843
31.866990	399.153083	4.531469	-0.006171	1.292289
31.956296	407.686633	4.536474	-0.006193	1.301633
32.356297	416.214105	4.541478	-0.006273	1.310960
33.101869	424.661334	4.546483	-0.006417	1.320197
33.790272	433.024500	4.551488	-0.006551	1.329270
34.452383	441.424854	4.556493	-0.006680	1.338315
35.222348	449.773148	4.561498	-0.006829	1.347264
35.739301	458.168779	4.566502	-0.006931	1.356159
35.988671	466.596916	4.571507	-0.006983	1.364983
36.441578	474.973929	4.576512	-0.007073	1.373732
37.161340	483.310118	4.581517	-0.007212	1.382430
37.577306	491.710097	4.586522	-0.007295	1.391086
37.888575	500.088294	4.591526	-0.007359	1.399649
38.247369	508.449858	4.596531	-0.007431	1.408151
39.088398	516.726855	4.601536	-0.007593	1.416597
39.817613	525.027954	4.606541	-0.007734	1.424998
40.359383	533.371708	4.611546	-0.007841	1.433362
40.668385	541.702393	4.616550	-0.007904	1.441626
41.493913	549.969293	4.621555	-0.008063	1.449863
41.963302	558.289449	4.626560	-0.008156	1.458048
42.418909	566.594909	4.631565	-0.008246	1.466171
42.881257	574.951382	4.636570	-0.008338	1.474300
43.319677	583.229112	4.641574	-0.008425	1.482304
43.857367	591.499901	4.646579	-0.008531	1.490274
44.328291	599.779943	4.651584	-0.008624	1.498200
44.862340	608.030188	4.656589	-0.008729	1.506066
45.255614	616.327234	4.661594	-0.008807	1.513913
45.538324	624.592857	4.666598	-0.008866	1.521674
46.176974	632.833340	4.671603	-0.008990	1.529425
46.378468	641.133065	4.676608	-0.009033	1.537126
46.594213	649.406741	4.681613	-0.009079	1.544766
47.039594	657.669671	4.686618	-0.009167	1.552394
47.519039	665.883448	4.691622	-0.009262	1.559944
47.962609	674.108052	4.696627	-0.009350	1.567462
48.258897	682.352933	4.701632	-0.009410	1.574941
48.953967	690.525436	4.706637	-0.009545	1.582377
49.528372	698.732143	4.711642	-0.009658	1.589791
49.520616	707.029176	4.716646	-0.009662	1.597168
50.422179	715.170657	4.721651	-0.009835	1.604502
50.952258	723.377860	4.726656	-0.009939	1.611809
51.386601	731.605997	4.731661	-0.010025	1.619086
51.608927	739.845387	4.736666	-0.010072	1.626312
52.279457	748.075735	4.741670	-0.010203	1.633559
52.666649	756.284126	4.746675	-0.010280	1.640717
52.836374	764.496837	4.751680	-0.010317	1.647817
53.142725	772.711812	4.756685	-0.010380	1.654907
53.529581	780.889189	4.761690	-0.010457	1.661945
53.837951	789.082153	4.766694	-0.010520	1.668957
54.599441	797.221732	4.771699	-0.010667	1.675954
55.174748	805.355186	4.776704	-0.010780	1.682892
55.737107	813.528630	4.781709	-0.010890	1.689834
56.290714	821.711155	4.786714	-0.010998	1.696753
56.654625	829.897349	4.791718	-0.011071	1.703622
56.912510	838.128985	4.796723	-0.011125	1.710487
56.999514	846.346314	4.801728	-0.011147	1.717291
57.584359	854.482100	4.806733	-0.011261	1.724065
58.341452	862.595093	4.811738	-0.011407	1.730815
58.375976	870.826741	4.816742	-0.011419	1.737544
58.700262	879.002766	4.821747	-0.011485	1.744238
59.082422	887.156764	4.826752	-0.011561	1.750897
59.421926	895.336481	4.831757	-0.011630	1.757545
59.939501	903.459729	4.836762	-0.011732	1.764145
60.272145	911.615990	4.841766	-0.011799	1.770723
60.606559	919.805219	4.846771	-0.011867	1.777304
60.703691	927.980806	4.851776	-0.011890	1.783820
60.944703	936.173584	4.856781	-0.011941	1.790343
61.440926	944.339776	4.861786	-0.012038	1.796853
61.837319	952.439249	4.866790	-0.012118	1.803275
62.639572	960.515903	4.871795	-0.012272	1.809705
63.001153	968.671625	4.876800	-0.012345	1.816121
63.231240	976.834436	4.881805	-0.012393	1.822504
63.560261	984.990941	4.886810	-0.012460	1.828871
63.981668	993.129457	4.891814	-0.012544	1.835213
64.396996	1001.268054	4.896819	-0.012627	1.841533
64.785293	1009.386421	4.901824	-0.012704	1.847812
65.505949	1017.502776	4.906829	-0.012844	1.854107
66.072231	1025.615642	4.911834	-0.012955	1.860360
65.980145	1033.808075	4.916838	-0.012943	1.866576
66.542118	1041.957999	4.921843	-0.013053	1.872814
67.129189	1050.044421	4.926848	-0.013168	1.878987
67.619063	1058.142225	4.931853	-0.013264	1.885137
67.649368	1066.336921	4.936858	-0.013275	1.891287
67.877421	1074.476288	4.941862	-0.013323	1.897398
68.239641	1082.591806	4.946867	-0.013396	1.903486
68.581537	1090.715051	4.951872	-0.013465	1.909559
69.089693	1098.821636	4.956877	-0.013565	1.915618
69.362635	1106.952347	4.961882	-0.013621	1.921650
69.662253	1115.070004	4.966886	-0.013682	1.927657
70.181291	1123.192621	4.971891	-0.013784	1.933672
70.478514	1131.315320	4.976896	-0.013845	1.939644
71.075929	1139.389986	4.981901	-0.013962	1.945596
71.247392	1147.584287	4.986906	-0.013999	1.951570
71.581226	1155.714620	4.991910	-0.014067	1.957496
72.013625	1163.792624	4.996915	-0.014153	1.963378
72.038616	1171.931730	5.001920	-0.014163	1.969242
72.333463	1180.048391	5.006925	-0.014223	1.975102
72.865836	1188.116730	5.011930	-0.014327	1.980935
73.150547	1196.219631	5.016934	-0.014386	1.986749
73.531606	1204.345624	5.021939	-0.014462	1.992572
74.071714	1212.412229	5.026944	-0.014568	1.998353
74.257473	1220.531925	5.031949	-0.014608	2.004118
74.655114	1228.636092	5.036954	-0.014687	2.009877
74.876167	1236.763928	5.041958	-0.014734	2.015618
75.305941	1244.864084	5.046963	-0.014819	2.021344
75.424982	1252.981272	5.051968	-0.014847	2.027035
75.783174	1261.111764	5.056973	-0.014919	2.032743
76.588447	1269.154370	5.061978	-0.015074	2.038419
76.760369	1277.256612	5.066982	-0.015112	2.044057
77.116989	1285.372408	5.071987	-0.015183	2.049707
77.380726	1293.488686	5.076992	-0.015238	2.055332
77.641126	1301.583836	5.081997	-0.015292	2.060928
77.975012	1309.682518	5.087002	-0.015359	2.066517
78.165207	1317.798070	5.092006	-0.015400	2.072089
78.574066	1325.891456	5.097011	-0.015482	2.077652
78.859193	1333.961458	5.102016	-0.015540	2.083172
79.392798	1342.023968	5.107021	-0.015645	2.088697
79.747081	1350.143015	5.112026	-0.015716	2.094228
79.917850	1358.241610	5.117030	-0.015753	2.099712
80.197020	1366.355618	5.122035	-0.015811	2.105203
80.838615	1374.421766	5.127040	-0.015935	2.110683
81.633056	1382.512567	5.132045	-0.016089	2.116179
82.059465	1390.576926	5.137050	-0.016173	2.121608
82.137311	1398.684223	5.142054	-0.016193	2.127019
82.687537	1406.777144	5.147059	-0.016301	2.132451
82.792633	1414.890798	5.152064	-0.016326	2.137840
82.829476	1423.006430	5.157069	-0.016338	2.143211
83.332296	1431.062138	5.162074	-0.016437	2.148573
83.566704	1439.167403	5.167078	-0.016486	2.153928
84.223087	1447.213141	5.172083	-0.016614	2.159271
84.502459	1455.284507	5.177088	-0.016671	2.164582
84.824474	1463.384218	5.182093	-0.016737	2.169902
85.144290	1471.487346	5.187098	-0.016801	2.175212
85.344016	1479.570555	5.192102	-0.016844	2.180484
85.814681	1487.636356	5.197107	-0.016937	2.185757
86.072647	1495.745773	5.202112	-0.016990	2.191026
86.465687	1503.837448	5.207117	-0.017069	2.196283
87.029786	1511.870328	5.212122	-0.017179	2.201505
87.246554	1519.963065	5.217126	-0.017225	2.206722
87.422090	1528.082871	5.222131	-0.017263	2.211940
87.757340	1536.154836	5.227136	-0.017331	2.217129
88.312892	1544.198927	5.232141	-0.017440	2.222308
88.524576	1552.303190	5.237146	-0.017484	2.227483
88.605508	1560.421590	5.242150	-0.017505	2.232643
88.989636	1568.492353	5.247155	-0.017582	2.237787
89.424101	1576.531923	5.252160	-0.017668	2.242905
89.728995	1584.615148	5.257165	-0.017730	2.248027
90.189151	1592.696960	5.262170	-0.017821	2.253149
90.538118	1600.772086	5.267174	-0.017891	2.258247
90.985259	1608.826155	5.272179	-0.017980	2.263327
91.277528	1616.917826	5.277184	-0.018040	2.268407
91.782951	1625.026746	5.282189	-0.018139	2.273504
91.946286	1633.129294	5.287194	-0.018175	2.278556
92.039364	1641.186840	5.292198	-0.018198	2.283564
92.666536	1649.202822	5.297203	-0.018320	2.288580
92.970983	1657.284203	5.302208	-0.018382	2.293597
93.095321	1665.375757	5.307213	-0.018410	2.298595
93.628943	1673.396190	5.312218	-0.018515	2.303573
93.927252	1681.468570	5.317222	-0.018576	2.308552
94.154867	1689.596578	5.322227	-0.018624	2.313548
94.397970	1697.644823	5.327232	-0.018674	2.318486
95.230232	1705.633515	5.332237	-0.018835	2.323426
95.547293	1713.730133	5.337242	-0.018899	2.328379
95.842181	1721.831530	5.342246	-0.018959	2.333322
96.211050	1729.907275	5.347251	-0.019033	2.338245
96.596840	1737.955881	5.352256	-0.019111	2.343142
96.936042	1746.033079	5.357261	-0.019179	2.348043
97.346395	1754.141151	5.362266	-0.019261	2.352958
97.558335	1762.192808	5.367270	-0.019306	2.357812
97.740308	1770.277235	5.372275	-0.019345	2.362673
97.824472	1778.349804	5.377280	-0.019366	2.367510
98.110369	1786.416852	5.382285	-0.019424	2.372350
98.712984	1794.450272	5.387290	-0.019542	2.377185
98.880310	1802.510873	5.392294	-0.019579	2.381991
99.497444	1810.554118	5.397299	-0.019699	2.386813
99.872713	1818.627847	5.402304	-0.019774	2.391624
100.092508	1826.714745	5.407309	-0.019820	2.396421
100.742117	1834.721631	5.412314	-0.019947	2.401195
100.891832	1842.804644	5.417318	-0.019980	2.405965
101.234300	1850.902716	5.422323	-0.020049	2.410749
101.476473	1858.980825	5.427328	-0.020099	2.415505
101.872739	1867.038094	5.432333	-0.020178	2.420250
102.251690	1875.086980	5.437338	-0.020254	2.424980
102.492812	1883.162233	5.442342	-0.020305	2.429706
102.979819	1891.313949	5.447347	-0.020401	2.434485
103.516745	1899.301600	5.452352	-0.020506	2.439164
103.952610	1907.319286	5.457357	-0.020592	2.443843
104.223427	1915.403973	5.462362	-0.020648	2.448539
104.345148	1923.474069	5.467366	-0.020676	2.453207
104.968255	1931.509859	5.472371	-0.020798	2.457884
104.998916	1939.591633	5.477376	-0.020809	2.462534
105.165259	1947.656069	5.482381	-0.020845	2.467175
105.670281	1955.713315	5.487386	-0.020944	2.471828
105.927676	1963.774236	5.492390	-0.020998	2.476457
106.296934	1971.811818	5.497395	-0.021072	2.481071
106.752846	1979.845164	5.502400	-0.021162	2.485681
106.918759	1987.935327	5.507405	-0.021198	2.490294
107.311008	1996.006166	5.512410	-0.021277	2.494903
107.509394	2004.051250	5.517414	-0.021319	2.499475
107.946053	2012.105967	5.522419	-0.021405	2.504061
108.103807	2020.176961	5.527424	-0.021440	2.508628
108.537289	2028.263738	5.532429	-0.021526	2.513216
109.123644	2036.281260	5.537434	-0.021641	2.517766
109.345210	2044.318837	5.542438	-0.021687	2.522294
109.553759	2052.396367	5.547443	-0.021732	2.526835
109.868637	2060.450712	5.552448	-0.021796	2.531362
110.231683	2068.511593	5.557453	-0.021868	2.535889
110.602328	2076.572129	5.562458	-0.021943	2.540407
110.815088	2084.584438	5.567462	-0.021988	2.544880
111.411070	2092.639807	5.572467	-0.022104	2.549395
111.705517	2100.722890	5.577472	-0.022164	2.553896
111.956066	2108.758208	5.582477	-0.022216	2.558360
112.330082	2116.817330	5.587482	-0.022291	2.562838
112.255468	2124.894564	5.592486	-0.022283	2.567287
112.848767	2132.945531	5.597491	-0.022398	2.571760
113.218274	2141.005707	5.602496	-0.022473	2.576215
113.533512	2149.061807	5.607501	-0.022537	2.580656
113.819629	2157.122219	5.612506	-0.022595	2.585089
114.250416	2165.155434	5.617510	-0.022681	2.589510
114.569369	2173.400395	5.622515	-0.022746	2.594031
114.918775	2181.417546	5.627520	-0.022816	2.598422
115.293484	2189.402242	5.632525	-0.022891	2.602790
115.780049	2197.412602	5.637530	-0.022987	2.607172
115.935436	2205.443188	5.642534	-0.023021	2.611535
116.380523	2213.492754	5.647539	-0.023109	2.615921
116.682740	2221.515332	5.652544	-0.023171	2.620275
117.153963	2229.534078	5.657549	-0.023264	2.624631
117.461525	2237.593842	5.662554	-0.023327	2.628990
117.816099	2245.646575	5.667558	-0.023398	2.633342
118.124082	2253.706050	5.672563	-0.023461	2.637687
118.250693	2261.746989	5.677568	-0.023490	2.642003
118.404177	2269.796996	5.682573	-0.023524	2.646319
118.790323	2277.856404	5.687578	-0.023601	2.650647
119.015569	2285.897853	5.692582	-0.023648	2.654949
119.223742	2293.978048	5.697587	-0.023692	2.659263
119.759188	2301.982322	5.702592	-0.023797	2.663551
119.961940	2310.050794	5.707597	-0.023840	2.667844
120.227956	2318.135345	5.712602	-0.023895	2.672143
120.564665	2326.183761	5.717606	-0.023963	2.676420
121.053119	2334.200894	5.722611	-0.024060	2.680684
121.126313	2342.233728	5.727616	-0.024078	2.684923
121.473326	2350.276036	5.732621	-0.024148	2.689177
121.953304	2358.327206	5.737626	-0.024243	2.693438
122.224204	2366.371231	5.742630	-0.024299	2.697675
122.488708	2374.424063	5.747635	-0.024354	2.701909
122.636940	2382.466550	5.752640	-0.024386	2.706124
123.055008	2390.511001	5.757645	-0.024470	2.710350
123.305619	2398.584621	5.762650	-0.024522	2.714575
123.467023	2406.628761	5.767654	-0.024557	2.718772
123.893191	2414.653380	5.772659	-0.024642	2.722968
124.133136	2422.686826	5.777664	-0.024692	2.727151
124.526838	2430.742894	5.782669	-0.024770	2.731349
124.966351	2438.805573	5.787674	-0.024858	2.735547
125.203632	2446.844266	5.792678	-0.024907	2.739713
125.922772	2454.862207	5.797683	-0.025046	2.743892
126.469168	2462.874272	5.802688	-0.025153	2.748050
126.828216	2470.999795	5.807693	-0.025226	2.752249
127.080428	2479.098729	5.812698	-0.025278	2.756422
127.443184	2487.089258	5.817702	-0.025351	2.760539
127.798456	2495.118445	5.822707	-0.025422	2.764669
127.915472	2503.179686	5.827712	-0.025449	2.768796
128.089552	2511.243935	5.832717	-0.025487	2.772921
128.520493	2519.285541	5.837722	-0.025573	2.777044
128.701223	2527.287312	5.842726	-0.025612	2.781125
129.085853	2535.311773	5.847731	-0.025689	2.785224
129.055520	2543.406118	5.852736	-0.025688	2.789328
129.516812	2551.440204	5.857741	-0.025779	2.793424
129.872293	2559.484335	5.862746	-0.025851	2.797513
129.828651	2567.526345	5.867750	-0.025848	2.801571
130.410261	2575.526163	5.872755	-0.025962	2.805639
130.916215	2583.547219	5.877760	-0.026061	2.809707
131.268975	2591.601453	5.882765	-0.026132	2.813777
131.617674	2599.667395	5.887770	-0.026203	2.817846
131.926963	2607.690492	5.892774	-0.026266	2.821886
132.070907	2615.764063	5.897779	-0.026298	2.825936
132.256981	2623.814517	5.902784	-0.026338	2.829971
132.495814	2631.896247	5.907789	-0.026388	2.834018
132.852476	2639.932451	5.912794	-0.026459	2.838044
132.812858	2647.958544	5.917798	-0.026457	2.842037
133.311336	2655.967232	5.922803	-0.026555	2.846046
133.649576	2663.993589	5.927808	-0.026624	2.850048
133.908046	2672.056156	5.932813	-0.026677	2.854059
134.182095	2680.098797	5.937818	-0.026733	2.858055
134.526856	2688.107000	5.942822	-0.026803	2.862032
134.923104	2696.146732	5.947827	-0.026882	2.866022
135.064791	2704.214281	5.952832	-0.026914	2.870006
135.175421	2712.285163	5.957837	-0.026940	2.873984
135.803032	2720.274799	5.962842	-0.027062	2.877945
136.118325	2728.288850	5.967846	-0.027126	2.881896
136.514954	2736.328641	5.972851	-0.027205	2.885858
136.793955	2744.397197	5.977856	-0.027262	2.889822
137.013925	2752.452835	5.982861	-0.027309	2.893772
137.265524	2760.509717	5.987866	-0.027361	2.897718
137.473235	2768.549872	5.992870	-0.027405	2.901648
137.756355	2776.583134	5.997875	-0.027463	2.905574
138.159965	2784.634124	6.002880	-0.027543	2.909509
138.336706	2792.750048	6.007885	-0.027582	2.913458
138.886929	2800.787927	6.012890	-0.027689	2.917384
138.940075	2808.804069	6.017894	-0.027705	2.921268
139.475983	2816.769929	6.022899	-0.027810	2.925148
139.747903	2824.788303	6.027904	-0.027866	2.929034
139.910326	2832.855928	6.032909	-0.027901	2.932933
140.106224	2840.913889	6.037914	-0.027943	2.936823
140.495844	2848.897388	6.042918	-0.028021	2.940683
140.970588	2856.916878	6.047923	-0.028115	2.944559
141.122168	2864.987229	6.052928	-0.028148	2.948438
141.479118	2873.038383	6.057933	-0.028220	2.952313
142.112517	2881.077166	6.062938	-0.028343	2.956191
142.298117	2889.072174	6.067942	-0.028383	2.960020
142.590608	2897.119242	6.072947	-0.028443	2.963875
143.071904	2905.115489	6.077952	-0.028538	2.967710
143.252588	2913.182604	6.082957	-0.028577	2.971558
143.456806	2921.292616	6.087962	-0.028620	2.975422
143.636019	2929.293522	6.092966	-0.028659	2.979229
143.959589	2937.327030	6.097971	-0.028725	2.983054
144.203953	2945.381384	6.102976	-0.028775	2.986879
144.531500	2953.405044	6.107981	-0.028842	2.990689
145.022902	2961.478082	6.112986	-0.028939	2.994526
145.309257	2969.477985	6.117990	-0.028997	2.998313
145.628724	2977.489990	6.122995	-0.029062	3.002102
145.997463	2985.503809	6.128000	-0.029136	3.005890
146.043588	2993.549713	6.133005	-0.029150	3.009672
146.311603	3001.658506	6.138010	-0.029205	3.013490
146.451262	3009.687778	6.143014	-0.029236	3.017260
146.955515	3017.700599	6.148019	-0.029336	3.021035
147.194004	3025.715881	6.153024	-0.029385	3.024793
147.594238	3033.728521	6.158029	-0.029465	3.028553
148.026933	3041.785497	6.163034	-0.029551	3.032331
148.127854	3049.827296	6.168038	-0.029575	3.036080
148.379595	3057.847440	6.173043	-0.029627	3.039823
148.852109	3065.871718	6.178048	-0.029721	3.043573
149.199356	3073.899475	6.183053	-0.029791	3.047314
149.488581	3081.966150	6.188058	-0.029850	3.051066
149.551653	3090.043082	6.193062	-0.029867	3.054807
149.962569	3098.053916	6.198067	-0.029949	3.058529
150.129759	3106.095489	6.203072	-0.029985	3.062250
150.297823	3114.138039	6.208077	-0.030022	3.065966
150.825625	3122.151915	6.213082	-0.030126	3.069682
150.964628	3130.252497	6.218086	-0.030157	3.073414
151.325934	3138.286827	6.223091	-0.030229	3.077122
151.645936	3146.261684	6.228096	-0.030294	3.080797
151.944471	3154.266115	6.233101	-0.030355	3.084479
152.194430	3162.327461	6.238106	-0.030407	3.088181
152.459030	3170.345222	6.243110	-0.030462	3.091859
152.645007	3178.416112	6.248115	-0.030502	3.095553
152.753968	3186.435950	6.253120	-0.030527	3.099216
153.086881	3194.449875	6.258125	-0.030594	3.102882
153.670943	3202.475247	6.263130	-0.030709	3.106561
153.801925	3210.487372	6.268134	-0.030738	3.110208
153.971940	3218.578740	6.273139	-0.030775	3.113889
154.237327	3226.618674	6.278144	-0.030830	3.117546
154.844384	3234.593779	6.283149	-0.030948	3.121185
155.046863	3242.620426	6.288154	-0.030991	3.124825
155.332981	3250.631727	6.293158	-0.031050	3.128458
155.643798	3258.704753	6.298163	-0.031113	3.132115
155.935250	3266.756704	6.303168	-0.031173	3.135757
156.169197	3274.771062	6.308173	-0.031222	3.139376
156.557120	3282.797840	6.313178	-0.031299	3.143003
156.787143	3290.840417	6.318182	-0.031347	3.146626
156.960112	3298.881218	6.323187	-0.031385	3.150241
157.477108	3306.950985	6.328192	-0.031487	3.153880
157.849950	3314.952866	6.333197	-0.031561	3.157478
158.068706	3323.003394	6.338202	-0.031607	3.161087
158.303225	3330.955407	6.343206	-0.031656	3.164649
158.919636	3338.986228	6.348211	-0.031776	3.168258
158.921346	3347.072172	6.353216	-0.031782	3.171861
159.203089	3355.098400	6.358221	-0.031840	3.175445
159.630143	3363.112938	6.363226	-0.031925	3.179026
159.926418	3371.149202	6.368230	-0.031985	3.182608
160.106158	3379.186747	6.373235	-0.032024	3.186180
160.423094	3387.210515	6.378240	-0.032088	3.189749
160.735330	3395.248820	6.383245	-0.032152	3.193320
161.044487	3403.320601	6.388250	-0.032215	3.196901
161.454277	3411.305090	6.393254	-0.032296	3.200444
161.556987	3419.344546	6.398259	-0.032321	3.203994
161.736823	3427.403456	6.403264	-0.032360	3.207552
161.952416	3435.433281	6.408269	-0.032405	3.211095
162.360429	3443.461190	6.413274	-0.032486	3.214641
162.687530	3451.485098	6.418278	-0.032553	3.218178
162.942990	3459.528239	6.423283	-0.032605	3.221716
163.372436	3467.529247	6.428288	-0.032691	3.225239
163.513426	3475.593821	6.433293	-0.032722	3.228775
163.823778	3483.672352	6.438298	-0.032785	3.232319
163.935727	3491.748199	6.443302	-0.032812	3.235851
164.171106	3499.716290	6.448307	-0.032861	3.239336
164.494321	3507.705076	6.453312	-0.032926	3.242830
164.801460	3515.721344	6.458317	-0.032989	3.246332
165.453132	3523.722770	6.463322	-0.033115	3.249837
165.821435	3531.737487	6.468326	-0.033189	3.253333
166.184721	3539.778750	6.473331	-0.033262	3.256836
166.356113	3547.802354	6.478336	-0.033299	3.260320
166.687089	3555.841787	6.483341	-0.033366	3.263813
167.060146	3563.883301	6.488346	-0.033441	3.267306
167.388509	3571.909450	6.493350	-0.033508	3.270786
167.681171	3579.975044	6.498355	-0.033568	3.274278
168.178753	3587.992547	6.503360	-0.033665	3.277753
168.070035	3596.026841	6.508365	-0.033651	3.281209
168.570760	3604.022200	6.513370	-0.033749	3.284667
168.750735	3612.056375	6.518374	-0.033788	3.288126
168.910185	3620.123496	6.523379	-0.033823	3.291595
169.088072	3628.185186	6.528384	-0.033861	3.295059
169.540563	3636.155216	6.533389	-0.033951	3.298490
169.847416	3644.200702	6.538394	-0.034013	3.301944
169.997751	3652.199917	6.543398	-0.034047	3.305369
170.630586	3660.235160	6.548403	-0.034170	3.308824
170.777040	3668.299239	6.553408	-0.034203	3.312269
170.969885	3676.346457	6.558413	-0.034244	3.315705
171.183642	3684.369469	6.563418	-0.034289	3.319128
171.427339	3692.360055	6.568422	-0.034340	3.322535
171.745922	3700.373758	6.573427	-0.034404	3.325950
171.972960	3708.397205	6.578432	-0.034452	3.329363
172.280575	3716.445583	6.583437	-0.034514	3.332786
172.659775	3724.502089	6.588442	-0.034590	3.336212
172.741180	3732.494607	6.593446	-0.034611	3.339596
173.041227	3740.542200	6.598451	-0.034672	3.343007
173.518787	3748.550329	6.603456	-0.034766	3.346405
173.857646	3756.572081	6.608461	-0.034835	3.349801
174.253150	3764.648448	6.613466	-0.034914	3.353217
174.302162	3772.700525	6.618470	-0.034928	3.356608
174.643161	3780.675691	6.623475	-0.034997	3.359973
174.917852	3788.695900	6.628480	-0.035053	3.363351
175.209275	3796.699814	6.633485	-0.035113	3.366720
175.518777	3804.770721	6.638490	-0.035176	3.370114
175.512586	3812.838553	6.643494	-0.035180	3.373492
175.950766	3820.851624	6.648499	-0.035267	3.376859
176.231946	3828.847994	6.653504	-0.035325	3.380211
176.354520	3836.874729	6.658509	-0.035353	3.383566
176.722843	3844.932364	6.663514	-0.035427	3.386939
176.942071	3852.941694	6.668518	-0.035473	3.390284
177.160583	3861.073174	6.673523	-0.035519	3.393676
177.527114	3869.070638	6.678528	-0.035592	3.397014
177.792144	3877.028922	6.683533	-0.035647	3.400329
177.963249	3885.037499	6.688538	-0.035684	3.403658
178.083365	3893.077803	6.693542	-0.035712	3.406996
178.357120	3901.080975	6.698547	-0.035768	3.410320
178.380569	3909.138320	6.703552	-0.035778	3.413654
178.612530	3917.173628	6.708557	-0.035826	3.416984
179.022169	3925.186482	6.713562	-0.035908	3.420306
179.380727	3933.137294	6.718566	-0.035980	3.423598
179.628942	3941.244361	6.723571	-0.036032	3.426948
179.980506	3949.277512	6.728576	-0.036102	3.430267
180.118012	3957.289627	6.733581	-0.036133	3.433568
180.508611	3965.345328	6.738586	-0.036211	3.436891
180.595399	3973.304154	6.743590	-0.036233	3.440161
180.777901	3981.349725	6.748595	-0.036272	3.443467
181.164448	3989.376853	6.753600	-0.036350	3.446769
181.243894	3997.401329	6.758605	-0.036370	3.450056
181.635455	4005.466648	6.763610	-0.036448	3.453368
182.028901	4013.502289	6.768614	-0.036526	3.456664
182.483064	4021.485109	6.773619	-0.036616	3.459937
182.606983	4029.524074	6.778624	-0.036645	3.463219
182.644314	4037.567603	6.783629	-0.036657	3.466497
183.231182	4045.588515	6.788634	-0.036772	3.469780
183.601427	4053.621275	6.793638	-0.036846	3.473058
183.919726	4061.667415	6.798643	-0.036910	3.476337
184.133538	4069.637124	6.803648	-0.036956	3.479578
184.623594	4077.634420	6.808653	-0.037052	3.482837
184.958369	4085.677740	6.813658	-0.037120	3.486105
185.294036	4093.683166	6.818662	-0.037188	3.489356
185.459210	4101.772768	6.823667	-0.037224	3.492632
185.682926	4109.809854	6.828672	-0.037271	3.495885
186.128387	4117.778636	6.833677	-0.037359	3.499115
186.533721	4125.816180	6.838682	-0.037440	3.502368
186.780688	4133.819248	6.843686	-0.037491	3.505599
186.972877	4141.874368	6.848691	-0.037532	3.508847
187.294101	4149.915558	6.853696	-0.037597	3.512089
187.605782	4157.936290	6.858701	-0.037661	3.515321
187.841556	4165.974981	6.863706	-0.037710	3.518554
188.078019	4173.966597	6.868710	-0.037759	3.521765
188.326090	4181.972545	6.873715	-0.037811	3.524980
188.787051	4190.019073	6.878720	-0.037902	3.528214
188.757202	4198.064732	6.883725	-0.037902	3.531430
189.184167	4206.119491	6.888730	-0.037986	3.534660
189.262809	4214.149132	6.893734	-0.038006	3.537867
189.446745	4222.140661	6.898739	-0.038046	3.541059
189.970272	4230.170724	6.903744	-0.038149	3.544273
190.232453	4238.179812	6.908749	-0.038203	3.547469
190.478782	4246.264187	6.913754	-0.038254	3.550690
190.632868	4254.355747	6.918758	-0.038288	3.553910
190.806364	4262.350995	6.923763	-0.038326	3.557088
191.102840	4270.333442	6.928768	-0.038386	3.560262
191.183320	4278.320810	6.933773	-0.038407	3.563429
191.505210	4286.336394	6.938778	-0.038472	3.566611
191.649288	4294.353263	6.943782	-0.038504	3.569786
191.970428	4302.411144	6.948787	-0.038569	3.572979
192.209944	4310.454597	6.953792	-0.038619	3.576162
192.563300	4318.410018	6.958797	-0.038690	3.579310
192.814699	4326.445725	6.963802	-0.038742	3.582483
192.822723	4334.479161	6.968806	-0.038749	3.585647
193.251005	4342.509498	6.973811	-0.038834	3.588818
193.601357	4350.529652	6.978816	-0.038905	3.591980
193.759205	4358.538119	6.983821	-0.038939	3.595129
194.059061	4366.573072	6.988826	-0.039001	3.598289
194.310166	4374.591589	6.993830	-0.039053	3.601440
194.451497	4382.569962	6.998835	-0.039084	3.604568
194.783145	4390.645720	7.003840	-0.039151	3.607737
195.004751	4398.671743	7.008845	-0.039198	3.610881
195.452870	4406.708219	7.013850	-0.039287	3.614032
195.837462	4414.721136	7.018854	-0.039364	3.617170
196.021641	4422.714277	7.023859	-0.039403	3.620292
196.347674	4430.755079	7.028864	-0.039469	3.623433
196.328435	4438.808435	7.033869	-0.039471	3.626567
196.650981	4446.816276	7.038874	-0.039536	3.629690
196.960005	4454.862642	7.043878	-0.039599	3.632825
197.285798	4462.915760	7.048883	-0.039665	3.635960
197.519678	4470.919461	7.053888	-0.039714	3.639071
197.580308	4478.926620	7.058893	-0.039731	3.642176
197.951948	4486.897728	7.063898	-0.039805	3.645272
197.994473	4494.957834	7.068902	-0.039818	3.648392
198.198907	4503.021195	7.073907	-0.039862	3.651514
198.638619	4511.053062	7.078912	-0.039949	3.654628
198.658504	4519.070007	7.083917	-0.039958	3.657722
198.851025	4527.093534	7.088922	-0.039999	3.660820
199.151688	4535.069706	7.093926	-0.040060	3.663901
199.368308	4543.098090	7.098931	-0.040106	3.666997
199.663940	4551.153294	7.103936	-0.040167	3.670102
199.859216	4559.187152	7.108941	-0.040208	3.673194
200.210560	4567.249302	7.113946	-0.040279	3.676298
200.344556	4575.204903	7.118950	-0.040309	3.679354
200.717316	4583.233822	7.123955	-0.040384	3.682440
200.952197	4591.277040	7.128960	-0.040433	3.685526
201.232636	4599.260473	7.133965	-0.040491	3.688588
201.431994	4607.318031	7.138970	-0.040533	3.691674
201.529513	4615.321165	7.143974	-0.040556	3.694733
201.986389	4623.325762	7.148979	-0.040647	3.697800
202.313259	4631.359514	7.153984	-0.040713	3.700871
202.328583	4639.354531	7.158989	-0.040721	3.703918
202.836589	4647.391866	7.163994	-0.040821	3.706990
202.795596	4655.417781	7.168998	-0.040819	3.710043
203.162804	4663.528677	7.174003	-0.040893	3.713134
203.477355	4671.567604	7.179008	-0.040956	3.716195
203.818718	4679.498843	7.184013	-0.041025	3.719212
203.996789	4687.563955	7.189018	-0.041064	3.722275
204.291651	4695.487470	7.194022	-0.041124	3.725283
204.643549	4703.518747	7.199027	-0.041195	3.728332
204.763625	4711.577847	7.204032	-0.041222	3.731382
205.047194	4719.595405	7.209037	-0.041281	3.734419
205.217755	4727.658069	7.214042	-0.041318	3.737467
205.483834	4735.631252	7.219046	-0.041372	3.740481
205.766450	4743.681225	7.224051	-0.041430	3.743523
205.810272	4751.756704	7.229056	-0.041444	3.746565
205.780297	4759.714665	7.234061	-0.041444	3.749560
206.113568	4767.802138	7.239066	-0.041511	3.752609
206.481425	4775.798647	7.244070	-0.041585	3.755622
206.696518	4783.780238	7.249075	-0.041630	3.758623
206.899215	4791.853151	7.254080	-0.041673	3.761656
207.234196	4799.796381	7.259085	-0.041741	3.764641
207.498403	4807.847890	7.264090	-0.041795	3.767663
207.751125	4815.898330	7.269094	-0.041848	3.770681
208.131971	4823.922631	7.274099	-0.041924	3.773690
208.531214	4831.967465	7.279104	-0.042004	3.776704
208.800179	4839.939630	7.284109	-0.042059	3.779687
208.962524	4847.988151	7.289114	-0.042095	3.782692
208.950448	4856.015723	7.294118	-0.042098	3.785684
209.244137	4864.038401	7.299123	-0.042158	3.788679
209.537014	4872.098663	7.304128	-0.042218	3.791684
209.719542	4880.103018	7.309133	-0.042257	3.794665
210.229294	4888.098093	7.314138	-0.042357	3.797646
210.123555	4896.126928	7.319142	-0.042343	3.800625
210.601799	4904.089574	7.324147	-0.042437	3.803589
210.984850	4912.153442	7.329152	-0.042514	3.806586
211.240656	4920.135004	7.334157	-0.042567	3.809547
211.437088	4928.216591	7.339162	-0.042609	3.812542
211.488686	4936.218278	7.344166	-0.042624	3.815502
211.682187	4944.216465	7.349171	-0.042665	3.818462
211.880508	4952.259588	7.354176	-0.042707	3.821435
212.065555	4960.240398	7.359181	-0.042747	3.824383
212.465629	4968.306033	7.364186	-0.042827	3.827365
212.780393	4976.314233	7.369190	-0.042891	3.830321
212.693998	4984.363018	7.374195	-0.042880	3.833282
213.068833	4992.394061	7.379200	-0.042955	3.836243
213.315581	5000.358683	7.384205	-0.043006	3.839175
213.526258	5008.412301	7.389210	-0.043051	3.842136
213.720107	5016.400804	7.394214	-0.043092	3.845071
213.886672	5024.414886	7.399219	-0.043129	3.848013
214.163476	5032.475198	7.404224	-0.043185	3.850971
214.384010	5040.481762	7.409229	-0.043232	3.853907
214.628651	5048.547019	7.414234	-0.043283	3.856862
215.002510	5056.527856	7.419238	-0.043358	3.859786
215.084799	5064.540865	7.424243	-0.043378	3.862714
215.415458	5072.558663	7.429248	-0.043445	3.865647
215.617314	5080.602428	7.434253	-0.043488	3.868584
215.947655	5088.636135	7.439258	-0.043555	3.871518
216.043788	5096.930401	7.444262	-0.043578	3.874539
216.378714	5104.852019	7.449267	-0.043646	3.877428
216.696689	5112.773714	7.454272	-0.043710	3.880314
216.865803	5120.733327	7.459277	-0.043747	3.883208
217.273265	5128.738994	7.464282	-0.043828	3.886122
217.451453	5136.733507	7.469286	-0.043867	3.889025
217.629755	5144.792668	7.474291	-0.043905	3.891950
217.991438	5152.831258	7.479296	-0.043978	3.894868
217.896735	5160.843423	7.484301	-0.043966	3.897766
218.264750	5168.839533	7.489306	-0.044039	3.900664
218.494910	5176.828050	7.494310	-0.044088	3.903555
218.923172	5184.856633	7.499315	-0.044173	3.906462
219.009107	5192.906133	7.504320	-0.044194	3.909368
219.196545	5200.929692	7.509325	-0.044234	3.912264
219.457454	5208.972930	7.514330	-0.044288	3.915167
219.835455	5216.967812	7.519334	-0.044364	3.918052
220.129633	5224.929529	7.524339	-0.044424	3.920921
220.375525	5232.906560	7.529344	-0.044475	3.923793
220.596624	5240.969025	7.534349	-0.044522	3.926693
220.757687	5249.005709	7.539354	-0.044557	3.929581
221.125757	5257.068696	7.544358	-0.044631	3.932479
221.245592	5265.088064	7.549363	-0.044658	3.935356
221.451277	5273.108306	7.554368	-0.044702	3.938232
221.550892	5281.103869	7.559373	-0.044726	3.941095
221.860031	5289.124871	7.564378	-0.044789	3.943969
222.101523	5297.131519	7.569382	-0.044839	3.946834
221.988136	5305.204826	7.574387	-0.044823	3.949715
222.201746	5313.221125	7.579392	-0.044868	3.952579
222.433401	5321.238976	7.584397	-0.044917	3.955442
222.548600	5329.250721	7.589402	-0.044943	3.958299
222.744347	5337.228553	7.594406	-0.044985	3.961142
222.976797	5345.213997	7.599411	-0.045034	3.963987
223.328028	5353.282307	7.604416	-0.045105	3.966862
223.176434	5361.268380	7.609421	-0.045082	3.969697
223.465156	5369.344389	7.614426	-0.045141	3.972569
223.905294	5377.363045	7.619430	-0.045228	3.975421
223.925937	5385.369043	7.624435	-0.045237	3.978259
224.238211	5393.415043	7.629440	-0.045301	3.981114
224.351939	5401.375427	7.634445	-0.045327	3.983934
224.369242	5409.437698	7.639450	-0.045336	3.986787
224.545083	5417.443821	7.644454	-0.045374	3.989619
225.046850	5425.504724	7.649459	-0.045472	3.992475
225.295906	5433.551077	7.654464	-0.045524	3.995319
225.242342	5441.545929	7.659469	-0.045520	3.998138
225.603560	5449.567879	7.664474	-0.045592	4.000971
225.733889	5457.560653	7.669478	-0.045622	4.003789
225.969273	5465.553613	7.674483	-0.045671	4.006606
226.265162	5473.587838	7.679488	-0.045731	4.009436
226.662688	5481.618113	7.684493	-0.045811	4.012265
226.840982	5489.649514	7.689498	-0.045849	4.015088
226.922337	5497.652574	7.694502	-0.045870	4.017898
227.149264	5505.651460	7.699507	-0.045917	4.020707
227.518517	5513.698071	7.704512	-0.045991	4.023533
227.593686	5521.709526	7.709517	-0.046010	4.026340
227.782788	5529.736950	7.714522	-0.046051	4.029152
228.115160	5537.819389	7.719526	-0.046118	4.031984
228.575909	5545.907630	7.724531	-0.046209	4.034817
228.569166	5553.871068	7.729536	-0.046213	4.037598
228.712994	5561.809575	7.734541	-0.046245	4.040371
228.927923	5569.860802	7.739546	-0.046291	4.043182
229.109851	5577.819623	7.744550	-0.046330	4.045958
229.233290	5585.857235	7.749555	-0.046358	4.048760
229.672216	5593.908233	7.754560	-0.046445	4.051568
229.814534	5601.896241	7.759565	-0.046477	4.054348
230.027602	5609.955233	7.764570	-0.046522	4.057152
230.296824	5617.906133	7.769574	-0.046578	4.059917
230.473321	5625.934675	7.774579	-0.046616	4.062706
230.583577	5633.958848	7.779584	-0.046642	4.065490
230.649863	5641.985814	7.784589	-0.046659	4.068273
231.209868	5649.987113	7.789594	-0.046769	4.071052
231.316852	5658.047997	7.794598	-0.046794	4.073844
231.547636	5666.082539	7.799603	-0.046842	4.076626
231.905297	5674.058107	7.804608	-0.046914	4.079387
232.008297	5682.074400	7.809613	-0.046939	4.082157
232.124051	5690.054980	7.814618	-0.046966	4.084913
232.407658	5698.125127	7.819622	-0.047024	4.087701
232.600936	5706.134581	7.824627	-0.047065	4.090464
232.846523	5714.183826	7.829632	-0.047116	4.093240
232.806527	5722.209483	7.834637	-0.047114	4.096002
233.182667	5730.219505	7.839642	-0.047189	4.098762
233.272250	5738.192171	7.844646	-0.047211	4.101504
233.516217	5746.195401	7.849651	-0.047262	4.104256
233.791326	5754.268468	7.854656	-0.047319	4.107031
234.006261	5762.265570	7.859661	-0.047364	4.109777
234.286404	5770.352283	7.864666	-0.047421	4.112553
234.290344	5778.369830	7.869670	-0.047428	4.115299
234.585067	5786.363088	7.874675	-0.047488	4.118040
234.804127	5794.379123	7.879680	-0.047534	4.120785
234.754656	5802.394663	7.884685	-0.047530	4.123525
235.130832	5810.409544	7.889690	-0.047605	4.126268
235.419580	5818.395510	7.894694	-0.047664	4.128998
235.452364	5826.458118	7.899699	-0.047676	4.131749
235.815457	5834.528325	7.904704	-0.047749	4.134505
236.115281	5842.500873	7.909709	-0.047810	4.137226
236.401114	5850.504046	7.914714	-0.047868	4.139954
236.318045	5858.545481	7.919718	-0.047858	4.142690
236.576304	5866.544737	7.924723	-0.047912	4.145413
237.029292	5874.574922	7.929728	-0.048001	4.148147
237.244490	5882.571727	7.934733	-0.048047	4.150866
237.371952	5890.657791	7.939738	-0.048076	4.153611
237.672655	5898.648647	7.944742	-0.048137	4.156325
237.956259	5906.615018	7.949747	-0.048195	4.159028
238.285356	5914.652504	7.954752	-0.048262	4.161754
238.307675	5922.636258	7.959757	-0.048271	4.164457
238.533154	5930.697073	7.964762	-0.048319	4.167186
238.786171	5938.667228	7.969766	-0.048371	4.169884
238.966294	5946.744840	7.974771	-0.048410	4.172614
239.193430	5954.736593	7.979776	-0.048457	4.175315
239.300697	5962.754092	7.984781	-0.048483	4.178021
239.673829	5970.762888	7.989786	-0.048557	4.180725
239.715402	5978.806901	7.994790	-0.048571	4.183436
239.857729	5986.800148	7.999795	-0.048602	4.186129
240.148769	5994.842260	8.004800	-0.048662	4.188838
240.272597	6002.858638	8.009805	-0.048690	4.191536
240.552211	6010.976762	8.014810	-0.048748	4.194267
240.732833	6019.016832	8.019814	-0.048787	4.196969
240.962826	6026.925753	8.024819	-0.048835	4.199626
241.058526	6034.969510	8.029824	-0.048858	4.202325
240.981789	6042.841017	8.034829	-0.048849	4.204962
241.347440	6050.951391	8.039834	-0.048922	4.207683
241.482350	6058.915372	8.044838	-0.048953	4.210350
241.629259	6066.954126	8.049843	-0.048985	4.213041
241.675898	6075.002866	8.054848	-0.048999	4.215733
241.908795	6083.002804	8.059853	-0.049048	4.218408
242.024680	6091.073003	8.064858	-0.049075	4.221104
242.365712	6099.046554	8.069862	-0.049144	4.223768
242.446513	6107.050429	8.074867	-0.049164	4.226438
242.691072	6115.094170	8.079872	-0.049215	4.229121
242.710535	6123.085634	8.084877	-0.049224	4.231783
243.126654	6131.125597	8.089882	-0.049307	4.234463
243.150619	6139.200376	8.094886	-0.049317	4.237149
243.328224	6147.107006	8.099891	-0.049355	4.239779
243.555062	6155.191201	8.104896	-0.049402	4.242466
243.765395	6163.133386	8.109901	-0.049447	4.245105
244.021143	6171.176342	8.114906	-0.049500	4.247776
244.200567	6179.221784	8.119910	-0.049539	4.250445
244.321852	6187.231483	8.124915	-0.049566	4.253101
244.634784	6195.298772	8.129920	-0.049630	4.255775
244.747991	6203.273585	8.134925	-0.049656	4.258415
244.941806	6211.331589	8.139930	-0.049698	4.261082
245.050150	6219.303371	8.144934	-0.049723	4.263718
245.315871	6227.348953	8.149939	-0.049778	4.266378
245.564118	6235.371731	8.154944	-0.049830	4.269028
245.751032	6243.418171	8.159949	-0.049870	4.271685
245.824488	6251.484819	8.164954	-0.049889	4.274345
246.136102	6259.494775	8.169958	-0.049952	4.276987
246.430417	6267.417299	8.174963	-0.050012	4.279598
246.704806	6275.516082	8.179968	-0.050069	4.282265
246.724801	6283.422914	8.184973	-0.050078	4.284866
246.997029	6291.480603	8.189978	-0.050134	4.287517
247.262063	6299.550222	8.194982	-0.050188	4.290169
247.341866	6307.555069	8.199987	-0.050209	4.292798
247.635856	6315.622735	8.204992	-0.050269	4.295447
247.906138	6323.577942	8.209997	-0.050324	4.298057
248.009580	6331.595268	8.215002	-0.050349	4.300685
248.147207	6339.621546	8.220006	-0.050380	4.303314
248.405409	6347.599526	8.225011	-0.050433	4.305927
248.697715	6355.661917	8.230016	-0.050493	4.308566
248.946993	6363.630001	8.235021	-0.050545	4.311172
249.226250	6371.722822	8.240026	-0.050602	4.313818
249.593761	6379.743259	8.245030	-0.050676	4.316439
249.621415	6387.669736	8.250035	-0.050686	4.319025
250.028655	6395.761520	8.255040	-0.050767	4.321666
250.112299	6403.716663	8.260045	-0.050788	4.324259
250.310299	6411.702057	8.265050	-0.050830	4.326861
250.396000	6419.735915	8.270054	-0.050852	4.329476
250.587692	6427.808999	8.275059	-0.050893	4.332103
251.061386	6435.821816	8.280064	-0.050986	4.334711
250.935255	6443.845874	8.285069	-0.050968	4.337317
250.951143	6451.818040	8.290074	-0.050976	4.339906
251.244087	6459.870399	8.295078	-0.051036	4.342520
251.433036	6467.844043	8.300083	-0.051077	4.345107
251.676872	6475.907232	8.305088	-0.051127	4.347722
251.871575	6483.853861	8.310093	-0.051169	4.350297
252.228739	6491.978785	8.315098	-0.051241	4.352929
252.317496	6500.007583	8.320102	-0.051263	4.355527
252.535464	6507.961563	8.325107	-0.051308	4.358100
253.000323	6515.945805	8.330112	-0.051400	4.360682
252.936452	6523.981250	8.335117	-0.051394	4.363277
253.133953	6531.981966	8.340122	-0.051436	4.365860
253.468425	6540.018015	8.345126	-0.051503	4.368454
253.628239	6548.000020	8.350131	-0.051538	4.371027
253.801415	6556.094178	8.355136	-0.051576	4.373636
253.782245	6564.075271	8.360141	-0.051578	4.376205
254.124124	6572.068564	8.365146	-0.051647	4.378779
254.137696	6580.141120	8.370150	-0.051655	4.381375
254.471888	6588.115060	8.375155	-0.051722	4.383939
254.793323	6596.178611	8.380160	-0.051787	4.386531
254.951580	6604.156288	8.385165	-0.051822	4.389093
255.053786	6612.160028	8.390170	-0.051846	4.391661
255.399311	6620.227031	8.395174	-0.051916	4.394249
255.615596	6628.220042	8.400179	-0.051962	4.396811
255.724653	6636.212620	8.405184	-0.051987	4.399371
255.685835	6644.238479	8.410189	-0.051985	4.401940
256.269746	6652.228515	8.415194	-0.052099	4.404498
256.355719	6660.266891	8.420198	-0.052121	4.407068
256.538385	6668.239200	8.425203	-0.052160	4.409616
256.768395	6676.323112	8.430208	-0.052208	4.412198
257.041649	6684.349597	8.435213	-0.052264	4.414761
257.234056	6692.390799	8.440218	-0.052306	4.417326
257.467398	6700.360756	8.445222	-0.052354	4.419867
257.756612	6708.370920	8.450227	-0.052413	4.422420
257.946351	6716.418549	8.455232	-0.052454	4.424983
258.255911	6724.438932	8.460237	-0.052517	4.427536
258.516826	6732.457830	8.465242	-0.052571	4.430087
258.527334	6740.537705	8.470246	-0.052578	4.432655
258.779094	6748.537654	8.475251	-0.052631	4.435197
259.108778	6756.594467	8.480256	-0.052697	4.437756
259.053645	6764.506184	8.485261	-0.052692	4.440266
259.235860	6772.547576	8.490266	-0.052731	4.442816
259.624547	6780.528177	8.495270	-0.052809	4.445346
259.918198	6788.543180	8.500275	-0.052869	4.447886
260.120338	6796.595497	8.505280	-0.052912	4.450435
260.002388	6804.617581	8.510285	-0.052895	4.452972
260.529039	6812.664814	8.515290	-0.052999	4.455518
260.772619	6820.643803	8.520294	-0.053050	4.458040
260.698856	6828.623836	8.525299	-0.053041	4.460560
261.079142	6836.662044	8.530304	-0.053117	4.463098
261.288818	6844.634444	8.535309	-0.053162	4.465614
261.299810	6852.680769	8.540314	-0.053169	4.468150
261.503842	6860.694114	8.545318	-0.053212	4.470676
261.974563	6868.725399	8.550323	-0.053305	4.473206
262.186712	6876.784686	8.555328	-0.053350	4.475743
262.343188	6884.754824	8.560333	-0.053384	4.478250
262.587678	6892.773415	8.565338	-0.053435	4.480772
262.766495	6900.775334	8.570343	-0.053474	4.483286
262.869824	6908.772526	8.575347	-0.053498	4.485797
263.220040	6916.794075	8.580352	-0.053569	4.488316
263.483863	6924.813016	8.585357	-0.053623	4.490831
263.628831	6932.852459	8.590362	-0.053656	4.493352
263.864539	6940.902754	8.595367	-0.053705	4.495874
264.064959	6948.885129	8.600371	-0.053748	4.498374
264.040902	6956.922590	8.605376	-0.053748	4.500889
264.216767	6964.892213	8.610381	-0.053786	4.503382
264.460965	6972.881836	8.615386	-0.053837	4.505880
264.604445	6980.949656	8.620391	-0.053869	4.508401
264.767537	6988.930908	8.625395	-0.053905	4.510893
265.180253	6997.067164	8.630400	-0.053987	4.513433
265.181971	7005.083557	8.635405	-0.053993	4.515933
265.342242	7013.047343	8.640410	-0.054028	4.518416
265.335407	7021.029584	8.645415	-0.054032	4.520902
265.538454	7028.994985	8.650419	-0.054075	4.523383
265.749466	7037.019998	8.655424	-0.054120	4.525880
265.751056	7045.035569	8.660429	-0.054125	4.528373
266.075764	7053.046906	8.665434	-0.054191	4.530864
266.430316	7061.094812	8.670439	-0.054262	4.533365
266.427763	7069.156006	8.675443	-0.054267	4.535868
266.649429	7077.161290	8.680448	-0.054314	4.538352
266.905772	7085.116537	8.685453	-0.054367	4.540820
266.905164	7093.138714	8.690458	-0.054372	4.543306
267.015212	7101.147732	8.695463	-0.054398	4.545788
267.398846	7109.172280	8.700467	-0.054475	4.548273
267.518550	7117.214399	8.705472	-0.054502	4.550762
267.397779	7125.241567	8.710477	-0.054485	4.553244
267.635218	7133.238640	8.715482	-0.054535	4.555717
268.073967	7141.295174	8.720487	-0.054622	4.558206
268.068668	7149.250279	8.725491	-0.054626	4.560662
268.340103	7157.295003	8.730496	-0.054682	4.563145
268.569119	7165.288637	8.735501	-0.054730	4.565611
268.870140	7173.331112	8.740506	-0.054791	4.568091
268.802616	7181.347358	8.745511	-0.054784	4.570560
269.030789	7189.379591	8.750515	-0.054832	4.573034
269.489511	7197.433177	8.755520	-0.054922	4.575513
269.524259	7205.391361	8.760525	-0.054934	4.577961
269.777047	7213.404375	8.765530	-0.054987	4.580424
269.882175	7221.456499	8.770535	-0.055011	4.582899
270.058451	7229.413319	8.775539	-0.055050	4.585342
270.472695	7237.502536	8.780544	-0.055132	4.587825
270.507165	7245.480374	8.785549	-0.055144	4.590272
270.545380	7253.525640	8.790554	-0.055156	4.592739
270.519896	7261.574229	8.795559	-0.055157	4.595206
270.901519	7269.544664	8.800563	-0.055233	4.597647
271.256633	7277.559267	8.805568	-0.055305	4.600100
271.176566	7285.603522	8.810573	-0.055295	4.602561
271.349410	7293.537896	8.815578	-0.055332	4.604987
271.714285	7301.667815	8.820583	-0.055406	4.607472
271.758019	7309.558542	8.825587	-0.055419	4.609882
271.915858	7317.640783	8.830592	-0.055454	4.612349
272.339690	7325.677713	8.835597	-0.055538	4.614801
272.511706	7333.676640	8.840602	-0.055575	4.617240
272.574305	7341.671452	8.845607	-0.055592	4.619677
272.737280	7349.663566	8.850611	-0.055628	4.622112
272.870021	7357.678354	8.855616	-0.055658	4.624552
272.887943	7365.720736	8.860621	-0.055667	4.626999
273.158799	7373.736277	8.865626	-0.055722	4.629437
273.645897	7381.781469	8.870631	-0.055819	4.631882
273.525077	7389.777755	8.875635	-0.055801	4.634311
273.700171	7397.825490	8.880640	-0.055839	4.636755
274.061039	7405.782528	8.885645	-0.055912	4.639170
273.984153	7413.809105	8.890650	-0.055903	4.641604
274.106215	7421.798442	8.895655	-0.055931	4.644027
274.399149	7429.823642	8.900659	-0.055991	4.646458
274.883759	7437.861231	8.905664	-0.056086	4.648892
274.750638	7445.853959	8.910669	-0.056067	4.651311
274.937220	7453.897758	8.915674	-0.056107	4.653744
275.247565	7461.895861	8.920679	-0.056170	4.656162
275.440933	7469.864578	8.925683	-0.056211	4.658570
275.605762	7477.970712	8.930688	-0.056247	4.661019
275.723953	7485.966104	8.935693	-0.056275	4.663432
275.984187	7493.932361	8.940698	-0.056328	4.665836
276.224754	7502.016618	8.945703	-0.056378	4.668273
276.264389	7509.993108	8.950707	-0.056391	4.670677
276.716436	7518.097638	8.955712	-0.056481	4.673118
276.668246	7526.121371	8.960717	-0.056477	4.675534
276.903847	7534.127299	8.965722	-0.056526	4.677943
276.835675	7542.074085	8.970727	-0.056519	4.680334
276.993507	7550.060811	8.975731	-0.056553	4.682735
277.271005	7558.027643	8.980736	-0.056610	4.685128
277.490561	7566.074131	8.985741	-0.056657	4.687544
277.736525	7574.090738	8.990746	-0.056708	4.689950
277.891496	7582.131660	8.995751	-0.056742	4.692362
278.045200	7590.160115	9.000755	-0.056776	4.694769
278.296127	7598.188359	9.005760	-0.056828	4.697175
278.440960	7606.116712	9.010765	-0.056860	4.699549
278.567339	7614.212733	9.015770	-0.056889	4.701973
278.857499	7622.199658	9.020775	-0.056948	4.704362
279.069610	7630.164994	9.025779	-0.056993	4.706744
279.153944	7638.245039	9.030784	-0.057014	4.709159
279.336752	7646.251822	9.035789	-0.057053	4.711551
279.681662	7654.254917	9.040794	-0.057123	4.713940
279.777519	7662.328797	9.045799	-0.057146	4.716349
279.982912	7670.267689	9.050803	-0.057190	4.718717
280.539224	7678.276065	9.055808	-0.057299	4.721103
280.701813	7686.348501	9.060813	-0.057334	4.723508
280.784568	7694.333056	9.065818	-0.057355	4.725886
281.189676	7702.390221	9.070823	-0.057436	4.728284
281.315577	7710.390821	9.075827	-0.057464	4.730664
281.519450	7718.352288	9.080832	-0.057508	4.733031
281.473622	7726.434719	9.085837	-0.057505	4.735434
281.847169	7734.474644	9.090842	-0.057579	4.737821
282.080854	7742.481361	9.095847	-0.057628	4.740198
282.215074	7750.507827	9.100851	-0.057659	4.742580
282.543422	7758.444978	9.105856	-0.057725	4.744933
282.530642	7766.524132	9.110861	-0.057728	4.747329
282.531775	7774.512709	9.115866	-0.057733	4.749696
282.747124	7782.578673	9.120871	-0.057779	4.752084
282.922839	7790.613460	9.125875	-0.057817	4.754462
283.036914	7798.594540	9.130880	-0.057843	4.756824
283.086205	7806.581933	9.135885	-0.057858	4.759186
283.323153	7814.576940	9.140890	-0.057907	4.761548
283.622546	7822.590622	9.145895	-0.057968	4.763915
283.607536	7830.565927	9.150899	-0.057971	4.766270
284.005150	7838.600781	9.155904	-0.058050	4.768640
284.116612	7846.632487	9.160909	-0.058076	4.771009
284.329167	7854.650653	9.165914	-0.058121	4.773372
284.810510	7862.730910	9.170919	-0.058216	4.775751
284.714543	7870.684798	9.175923	-0.058204	4.778095
284.814849	7878.655096	9.180928	-0.058228	4.780441
284.967579	7886.700203	9.185933	-0.058261	4.782808
285.156384	7894.685161	9.190938	-0.058302	4.785155
285.299060	7902.788112	9.195943	-0.058334	4.787537
285.392542	7910.687136	9.200947	-0.058356	4.789857
285.770648	7918.839203	9.205952	-0.058432	4.792250
286.004683	7926.828242	9.210957	-0.058481	4.794594
286.167925	7934.878652	9.215962	-0.058517	4.796955
286.251532	7942.792263	9.220967	-0.058538	4.799275
286.432567	7950.819004	9.225971	-0.058577	4.801627
286.759462	7958.766992	9.230976	-0.058643	4.803954
286.787417	7966.847075	9.235981	-0.058653	4.806320
287.107856	7974.873350	9.240986	-0.058718	4.808667
287.318366	7982.899589	9.245991	-0.058763	4.811014
287.333612	7990.426492	9.250995	-0.058771	4.813215
287.689259	7995.062307	9.256000	-0.058840	4.814568

287.640210	7997.433251	9.261005	-0.058832	4.815261
287.728989	7998.651901	9.266010	-0.058850	4.815616
287.651957	7999.549181	9.271015	-0.058836	4.815879
287.819663	7999.774513	9.276019	-0.058868	4.815944
287.927349	7999.805335	9.281024	-0.058888	4.815952
287.867642	7999.772198	9.286029	-0.058877	4.815943
288.179130	7999.786426	9.291034	-0.058935	4.815946
288.284458	7999.787283	9.296039	-0.058955	4.815945
288.126802	7999.782285	9.301043	-0.058925	4.815945
288.154112	7999.812713	9.306048	-0.058931	4.815953
288.298136	7999.760843	9.311053	-0.058957	4.815937
288.510467	7999.796776	9.316058	-0.058997	4.815947
288.550876	7999.782560	9.321063	-0.059005	4.815942
288.742076	7999.762540	9.326067	-0.059040	4.815936
288.920025	7999.823496	9.331072	-0.059074	4.815952
288.838361	7999.776066	9.336077	-0.059058	4.815939
288.734109	7999.805167	9.341082	-0.059039	4.815948
289.012784	7999.815594	9.346087	-0.059091	4.815950
288.913359	7999.812723	9.351091	-0.059073	4.815949
289.100454	7999.812933	9.356096	-0.059108	4.815948
289.142453	7999.793402	9.361101	-0.059116	4.815942
289.160315	7999.799080	9.366106	-0.059119	4.815944
289.003103	7999.853933	9.371111	-0.059090	4.815961
289.014311	7999.814606	9.376115	-0.059092	4.815949
289.160240	7999.809791	9.381120	-0.059119	4.815947
289.217268	7999.770230	9.386125	-0.059130	4.815935
289.123498	7999.790973	9.391130	-0.059113	4.815942
289.339021	7999.798112	9.396135	-0.059153	4.815943
289.209095	7999.789343	9.401139	-0.059129	4.815941
289.267146	7999.839567	9.406144	-0.059140	4.815955
289.336244	7999.794882	9.411149	-0.059153	4.815942
289.431856	7999.809456	9.416154	-0.059170	4.815946
289.266105	7999.826751	9.421159	-0.059140	4.815951
289.369169	7999.785890	9.426163	-0.059159	4.815939
289.610424	7999.813804	9.431168	-0.059204	4.815946
289.520018	7999.801479	9.436173	-0.059187	4.815943
289.382174	7999.794703	9.441178	-0.059162	4.815941
289.458027	7999.803574	9.446183	-0.059176	4.815944
289.515853	7999.790743	9.451187	-0.059187	4.815940
289.448167	7999.829060	9.456192	-0.059174	4.815951
289.456590	7999.784338	9.461197	-0.059176	4.815938
289.634538	7999.807893	9.466202	-0.059209	4.815944
289.749851	7999.830307	9.471207	-0.059231	4.815950
289.556496	7999.800077	9.476211	-0.059195	4.815942
289.806789	7999.850598	9.481216	-0.059241	4.815956
289.757171	7999.801613	9.486221	-0.059232	4.815941
289.892236	7999.824387	9.491226	-0.059258	4.815947
290.015460	7999.809541	9.496231	-0.059281	4.815942
289.760345	7999.782461	9.501235	-0.059233	4.815936
289.759438	7999.813444	9.506240	-0.059233	4.815945
289.880222	7999.814585	9.511245	-0.059256	4.815945
289.903543	7999.809675	9.516250	-0.059260	4.815943
289.968932	7999.806600	9.521255	-0.059272	4.815942
289.989480	7999.778129	9.526259	-0.059276	4.815933
290.168998	7999.840186	9.531264	-0.059310	4.815951
290.249289	7999.793567	9.536269	-0.059325	4.815936
289.848838	7999.800173	9.541274	-0.059250	4.815941
290.154518	7999.827124	9.546279	-0.059307	4.815947
290.185732	7999.812740	9.551283	-0.059313	4.815942
290.272479	7999.845321	9.556288	-0.059330	4.815951
290.227771	7999.793219	9.561293	-0.059321	4.815936
290.411592	7999.838256	9.566298	-0.059356	4.815949
290.126395	7999.842686	9.571303	-0.059303	4.815951
290.066617	7999.807408	9.576307	-0.059292	4.815941
290.232867	7999.887391	9.581312	-0.059323	4.815964
290.171809	7999.858502	9.586317	-0.059311	4.815956
290.222936	7999.835931	9.591322	-0.059321	4.815949
290.239338	7999.839445	9.596327	-0.059324	4.815950
290.296658	7999.806300	9.601331	-0.059335	4.815940
290.317963	7999.846238	9.606336	-0.059339	4.815951
290.338335	7999.838069	9.611341	-0.059343	4.815949
290.246252	7999.825713	9.616346	-0.059326	4.815946
290.259499	7999.854818	9.621351	-0.059328	4.815954
290.388303	7999.825113	9.626355	-0.059352	4.815945
290.363984	7999.868495	9.631360	-0.059348	4.815958
290.571610	7999.818852	9.636365	-0.059387	4.815942
290.343290	7999.823250	9.641370	-0.059344	4.815945
290.543966	7999.850427	9.646375	-0.059382	4.815951
290.402544	7999.825416	9.651379	-0.059355	4.815945
290.500312	7999.830413	9.656384	-0.059374	4.815946
290.477063	7999.829998	9.661389	-0.059369	4.815946
290.474072	7999.835296	9.666394	-0.059369	4.815947
290.543597	7999.825884	9.671399	-0.059382	4.815944
290.394416	7999.809282	9.676403	-0.059354	4.815940
290.519909	7999.872493	9.681408	-0.059378	4.815958
290.546512	7999.828101	9.686413	-0.059383	4.815945
290.385233	7999.847614	9.691418	-0.059353	4.815951
290.509763	7999.856304	9.696423	-0.059376	4.815953
290.553652	7999.805815	9.701427	-0.059384	4.815938
290.482553	7999.838727	9.706432	-0.059371	4.815948
290.429945	7999.798236	9.711437	-0.059362	4.815937
290.512782	7999.847845	9.716442	-0.059377	4.815951
290.513342	7999.863894	9.721447	-0.059377	4.815956
290.491399	7999.812206	9.726451	-0.059373	4.815941
290.642245	7999.861986	9.731456	-0.059402	4.815954
290.689933	7999.834009	9.736461	-0.059410	4.815946
290.573769	7999.875718	9.741466	-0.059389	4.815959
290.519035	7999.858699	9.746471	-0.059379	4.815954
290.607844	7999.841089	9.751475	-0.059395	4.815948
290.670142	7999.852920	9.756480	-0.059407	4.815951
290.526598	7999.865275	9.761485	-0.059381	4.815956
290.695955	7999.828828	9.766490	-0.059412	4.815944
290.720066	7999.837826	9.771495	-0.059417	4.815947
290.607190	7999.807992	9.776499	-0.059396	4.815939
290.612372	7999.843362	9.781504	-0.059397	4.815949
290.791470	7999.808161	9.786509	-0.059430	4.815938
290.709002	7999.848347	9.791514	-0.059415	4.815950
290.665364	7999.887102	9.796519	-0.059407	4.815961
290.663772	7999.821891	9.801523	-0.059407	4.815942
290.756900	7999.835353	9.806528	-0.059424	4.815946
290.683945	7999.807315	9.811533	-0.059411	4.815938
290.633590	7999.826711	9.816538	-0.059401	4.815944
290.794724	7999.841412	9.821543	-0.059432	4.815947
290.741054	7999.812657	9.826547	-0.059422	4.815939
290.789142	7999.849878	9.831552	-0.059431	4.815950
291.022459	7999.817803	9.836557	-0.059474	4.815939
290.856087	7999.840428	9.841562	-0.059443	4.815947
290.773106	7999.817551	9.846567	-0.059428	4.815941
290.742593	7999.804179	9.851571	-0.059422	4.815937
290.762827	7999.843030	9.856576	-0.059426	4.815948
290.590070	7999.833479	9.861581	-0.059394	4.815946
290.650033	7999.823893	9.866586	-0.059405	4.815943
290.842674	7999.833825	9.871591	-0.059441	4.815945
290.655097	7999.784461	9.876595	-0.059406	4.815931
290.709428	7999.827139	9.881600	-0.059417	4.815944
290.713670	7999.824019	9.886605	-0.059418	4.815943
291.002858	7999.839985	9.891610	-0.059472	4.815946
290.857596	7999.849102	9.896615	-0.059445	4.815949
290.831694	7999.820853	9.901619	-0.059440	4.815941
290.877612	7999.924294	9.906624	-0.059449	4.815971
290.812661	7999.809837	9.911629	-0.059436	4.815938
290.962591	7999.837158	9.916634	-0.059465	4.815945
290.897903	7999.857362	9.921639	-0.059453	4.815951
290.749759	7999.821541	9.926643	-0.059425	4.815942
290.883653	7999.849639	9.931648	-0.059450	4.815949
290.975811	7999.825679	9.936653	-0.059467	4.815942
291.062368	7999.822990	9.941658	-0.059484	4.815941
290.918386	7999.825718	9.946663	-0.059457	4.815942
291.065441	7999.820926	9.951667	-0.059484	4.815940
291.063756	7999.864721	9.956672	-0.059484	4.815953
291.262079	7999.920712	9.961677	-0.059521	4.815968
291.197660	7999.834050	9.966682	-0.059509	4.815943
291.419106	7999.840232	9.971687	-0.059550	4.815944
291.216608	7999.832275	9.976691	-0.059513	4.815942
291.271201	7999.874959	9.981696	-0.059523	4.815955
291.184193	7999.834908	9.986701	-0.059507	4.815943
291.207222	7999.838543	9.991706	-0.059511	4.815944
291.138114	7999.841567	9.996711	-0.059499	4.815946
291.211606	7999.814060	10.001715	-0.059512	4.815937
291.235874	7999.838023	10.006720	-0.059517	4.815944
291.110679	7999.825063	10.011725	-0.059494	4.815941
291.131500	7999.845757	10.016730	-0.059498	4.815947
291.238943	7999.848792	10.021735	-0.059518	4.815947
291.080882	7999.817065	10.026739	-0.059488	4.815939
291.171768	7999.849723	10.031744	-0.059506	4.815948
291.208102	7999.832226	10.036749	-0.059512	4.815942
291.191582	7999.833002	10.041754	-0.059509	4.815943
291.209847	7999.857925	10.046759	-0.059513	4.815950
291.191448	7999.834086	10.051763	-0.059510	4.815943
291.368207	7999.950601	10.056768	-0.059543	4.815976
291.169815	7999.832641	10.061773	-0.059506	4.815943
291.198487	7999.840653	10.066778	-0.059511	4.815945
291.318893	7999.844994	10.071783	-0.059534	4.815946
291.309596	7999.810635	10.076787	-0.059532	4.815936
291.402990	7999.845476	10.081792	-0.059549	4.815945
291.524563	7999.853045	10.086797	-0.059572	4.815947
291.452357	7999.873112	10.091802	-0.059559	4.815953
291.337955	7999.905234	10.096807	-0.059538	4.815963
291.285043	7999.839087	10.101811	-0.059528	4.815944
291.458374	7999.894622	10.106816	-0.059560	4.815959
291.485344	7999.872680	10.111821	-0.059565	4.815953
291.348477	7999.841338	10.116826	-0.059540	4.815944
291.545130	7999.865237	10.121831	-0.059577	4.815950
291.489547	7999.836446	10.126835	-0.059566	4.815942
291.435491	7999.857913	10.131840	-0.059556	4.815949
291.632634	7999.854034	10.136845	-0.059593	4.815946
291.583847	7999.852085	10.141850	-0.059584	4.815946
291.469539	7999.857491	10.146855	-0.059563	4.815948
291.332989	7999.810125	10.151859	-0.059538	4.815935
291.470734	7999.883180	10.156864	-0.059563	4.815956
291.531767	7999.852240	10.161869	-0.059575	4.815946
291.345130	7999.863808	10.166874	-0.059540	4.815951
291.498132	7999.889049	10.171879	-0.059569	4.815957
291.525532	7999.871389	10.176883	-0.059574	4.815952
291.468834	7999.899220	10.181888	-0.059564	4.815961
291.544623	7999.858930	10.186893	-0.059578	4.815948
291.571140	7999.839117	10.191898	-0.059583	4.815942
291.600835	7999.862110	10.196903	-0.059588	4.815949
291.334852	7999.923531	10.201907	-0.059539	4.815968
291.488546	7999.848325	10.206912	-0.059568	4.815946
291.616931	7999.826094	10.211917	-0.059592	4.815938
291.429717	7999.837652	10.216922	-0.059557	4.815943
291.821330	7999.864037	10.221927	-0.059630	4.815948
291.829214	7999.875945	10.226931	-0.059631	4.815952
291.735791	7999.857151	10.231936	-0.059614	4.815947
291.722175	7999.844087	10.236941	-0.059612	4.815943
291.663101	7999.847294	10.241946	-0.059601	4.815944
291.619444	7999.853988	10.246951	-0.059593	4.815946
291.663364	7999.832354	10.251955	-0.059601	4.815940
291.566895	7999.853048	10.256960	-0.059583	4.815946
291.562837	7999.848708	10.261965	-0.059582	4.815945
291.499548	7999.835807	10.266970	-0.059571	4.815942
291.454841	7999.865994	10.271975	-0.059563	4.815951
291.592387	7999.816142	10.276979	-0.059588	4.815936
291.590731	7999.836427	10.281984	-0.059588	4.815941
291.670076	7999.828263	10.286989	-0.059603	4.815939
291.578080	7999.843695	10.291994	-0.059586	4.815944
291.575941	7999.859695	10.296999	-0.059586	4.815948
291.478683	7999.829076	10.302003	-0.059568	4.815940
291.633283	7999.861827	10.307008	-0.059596	4.815949
291.858083	7999.845629	10.312013	-0.059638	4.815943
291.808218	7999.844728	10.317018	-0.059629	4.815943
291.795688	7999.880845	10.322023	-0.059627	4.815953
291.764920	7999.827926	10.327027	-0.059621	4.815938
291.625426	7999.843560	10.332032	-0.059595	4.815943
291.515032	7999.845831	10.337037	-0.059575	4.815945
291.799586	7999.838203	10.342042	-0.059628	4.815941
291.816425	7999.888749	10.347047	-0.059631	4.815956
291.646269	7999.854662	10.352051	-0.059600	4.815946
291.715053	7999.877300	10.357056	-0.059613	4.815953
291.739729	7999.889514	10.362061	-0.059617	4.815956
291.755049	7999.880184	10.367066	-0.059620	4.815953
291.838652	7999.867823	10.372071	-0.059636	4.815949
291.744890	7999.834061	10.377075	-0.059618	4.815940
291.857721	7999.876739	10.382080	-0.059640	4.815952
291.786225	7999.940637	10.387085	-0.059626	4.815971
291.750361	7999.839531	10.392090	-0.059620	4.815941
291.793782	7999.817888	10.397095	-0.059628	4.815935
291.811494	7999.821426	10.402099	-0.059631	4.815936
291.871285	7999.868480	10.407104	-0.059643	4.815949
291.869210	7999.866314	10.412109	-0.059642	4.815949
291.697239	7999.849294	10.417114	-0.059610	4.815945
291.693402	7999.849233	10.422119	-0.059610	4.815945
291.774850	7999.838970	10.427123	-0.059625	4.815941
291.943806	7999.857022	10.432128	-0.059656	4.815946
291.818326	7999.850468	10.437133	-0.059633	4.815944
291.606543	7999.845547	10.442138	-0.059594	4.815944
291.831759	7999.852868	10.447143	-0.059636	4.815945
291.727468	7999.810364	10.452147	-0.059617	4.815933
291.827688	7999.878461	10.457152	-0.059635	4.815952
291.938828	7999.843090	10.462157	-0.059656	4.815941
291.868597	7999.852506	10.467162	-0.059643	4.815945
291.839555	7999.875498	10.472167	-0.059638	4.815951
291.983448	7999.823625	10.477171	-0.059665	4.815936
292.055671	7999.859150	10.482176	-0.059678	4.815946
291.919679	7999.862023	10.487181	-0.059653	4.815947
291.808511	7999.861073	10.492186	-0.059632	4.815947
292.000883	7999.888102	10.497191	-0.059668	4.815954
291.768483	7999.830437	10.502195	-0.059625	4.815939
291.892886	7999.882944	10.507200	-0.059648	4.815953
291.892294	7999.839124	10.512205	-0.059648	4.815941
291.748795	7999.853616	10.517210	-0.059622	4.815946
291.861024	7999.866359	10.522215	-0.059643	4.815949
292.102746	7999.850469	10.527219	-0.059688	4.815943
291.984868	7999.895353	10.532224	-0.059666	4.815956
291.794439	7999.844865	10.537229	-0.059631	4.815943
291.960532	7999.835078	10.542234	-0.059662	4.815939
292.065033	7999.862641	10.547239	-0.059681	4.815946
291.864238	7999.832271	10.552243	-0.059644	4.815939
291.984817	7999.952039	10.557248	-0.059666	4.815973
292.239873	7999.831656	10.562253	-0.059714	4.815936
291.899907	7999.840429	10.567258	-0.059651	4.815941
292.060809	7999.928870	10.572263	-0.059681	4.815966
291.989774	7999.876284	10.577267	-0.059668	4.815951
291.970424	7999.862047	10.582272	-0.059664	4.815947
292.147221	7999.840698	10.587277	-0.059697	4.815940
292.052043	7999.851797	10.592282	-0.059680	4.815943
291.993863	7999.876394	10.597287	-0.059669	4.815951
292.030226	7999.827904	10.602291	-0.059676	4.815936
292.012273	7999.848960	10.607296	-0.059672	4.815943
292.067206	7999.854246	10.612301	-0.059683	4.815944
292.024429	7999.849200	10.617306	-0.059675	4.815943
291.961084	7999.867291	10.622311	-0.059663	4.815948
291.963905	7999.888726	10.627315	-0.059664	4.815955
292.187500	7999.879987	10.632320	-0.059705	4.815951
292.077285	7999.898292	10.637325	-0.059685	4.815957
291.906841	7999.886643	10.642330	-0.059653	4.815954
292.245791	7999.869320	10.647335	-0.059717	4.815947
292.189979	7999.860830	10.652339	-0.059706	4.815945
292.085532	7999.870690	10.657344	-0.059687	4.815949
292.189004	7999.833043	10.662349	-0.059706	4.815937
292.180878	7999.838247	10.667354	-0.059705	4.815939
291.871966	7999.874304	10.672359	-0.059647	4.815951
291.894834	7999.864042	10.677363	-0.059652	4.815948
292.078033	7999.862048	10.682368	-0.059686	4.815946
292.045840	7999.834751	10.687373	-0.059680	4.815938
292.103060	7999.837941	10.692378	-0.059691	4.815939
292.179014	7999.855366	10.697383	-0.059705	4.815944
292.216725	7999.848581	10.702387	-0.059712	4.815941
292.112008	7999.927905	10.707392	-0.059693	4.815965
292.107770	7999.840200	10.712397	-0.059692	4.815940
292.188297	7999.845952	10.717402	-0.059707	4.815941
292.288248	7999.863814	10.722407	-0.059726	4.815946
292.225509	7999.835960	10.727411	-0.059714	4.815938
292.326444	7999.879491	10.732416	-0.059733	4.815950
292.237898	7999.897122	10.737421	-0.059717	4.815956
292.119158	7999.866110	10.742426	-0.059695	4.815947
292.237585	7999.889653	10.747431	-0.059717	4.815953
292.072701	7999.823600	10.752435	-0.059686	4.815935
292.235344	7999.856499	10.757440	-0.059717	4.815944
292.254844	7999.850451	10.762445	-0.059720	4.815942
292.348174	7999.851093	10.767450	-0.059738	4.815941
292.254138	7999.880380	10.772455	-0.059720	4.815951
292.001463	7999.829826	10.777459	-0.059673	4.815937
292.415268	7999.870511	10.782464	-0.059751	4.815947
292.237118	7999.859790	10.787469	-0.059718	4.815945
292.111432	7999.859645	10.792474	-0.059694	4.815945
292.258941	7999.867687	10.797479	-0.059722	4.815947
292.218892	7999.846660	10.802483	-0.059714	4.815941
292.367508	7999.882509	10.807488	-0.059742	4.815951
292.246995	7999.886733	10.812493	-0.059720	4.815952
292.226519	7999.872475	10.817498	-0.059716	4.815948
292.320807	7999.891303	10.822503	-0.059734	4.815953
292.155153	7999.850885	10.827507	-0.059703	4.815942
292.179010	7999.880185	10.832512	-0.059708	4.815951
292.189038	7999.870758	10.837517	-0.059709	4.815948
292.037268	7999.853037	10.842522	-0.059681	4.815944
292.274829	7999.910815	10.847527	-0.059726	4.815959
292.256569	7999.862397	10.852531	-0.059722	4.815945
292.243990	7999.852558	10.857536	-0.059720	4.815942
292.215325	7999.827463	10.862541	-0.059715	4.815935
292.283776	7999.847957	10.867546	-0.059728	4.815941
292.393236	7999.865993	10.872551	-0.059748	4.815946
292.186266	7999.863297	10.877555	-0.059710	4.815946
292.274574	7999.876672	10.882560	-0.059726	4.815949
292.500522	7999.891489	10.887565	-0.059768	4.815952
292.375690	7999.879603	10.892570	-0.059745	4.815950
292.339126	7999.903526	10.897575	-0.059739	4.815957
292.255254	7999.947961	10.902579	-0.059723	4.815970
292.615098	7999.911783	10.907584	-0.059790	4.815958
292.259750	7999.898898	10.912589	-0.059724	4.815956
292.279310	7999.875752	10.917594	-0.059728	4.815949
292.516912	7999.899331	10.922599	-0.059772	4.815955
292.438486	7999.832716	10.927603	-0.059758	4.815936
292.301087	7999.863350	10.932608	-0.059732	4.815945
292.413694	7999.857931	10.937613	-0.059753	4.815943
292.352905	7999.879275	10.942618	-0.059742	4.815950
292.349468	7999.877084	10.947623	-0.059741	4.815949
292.419199	7999.846302	10.952627	-0.059754	4.815940
292.448815	7999.846851	10.957632	-0.059760	4.815940
292.340191	7999.837398	10.962637	-0.059740	4.815937
292.357532	7999.856960	10.967642	-0.059743	4.815943
292.450506	7999.861871	10.972647	-0.059761	4.815944
292.247589	7999.853904	10.977651	-0.059723	4.815943
292.189873	7999.850723	10.982656	-0.059712	4.815942
292.552594	7999.882996	10.987661	-0.059780	4.815950
292.385354	7999.846824	10.992666	-0.059749	4.815940
292.186101	7999.854956	10.997671	-0.059712	4.815943
292.152088	7999.830832	11.002675	-0.059706	4.815936
292.252870	7999.858328	11.007680	-0.059724	4.815944
292.344384	7999.853594	11.012685	-0.059742	4.815942
292.342033	7999.848216	11.017690	-0.059741	4.815941
292.586881	7999.897577	11.022695	-0.059787	4.815954
292.547816	7999.872292	11.027699	-0.059780	4.815946
292.580157	7999.910297	11.032704	-0.059786	4.815957
292.489261	7999.895823	11.037709	-0.059769	4.815954
292.479338	7999.875345	11.042714	-0.059767	4.815948
292.563806	7999.915369	11.047719	-0.059783	4.815959
292.479325	7999.894600	11.052723	-0.059767	4.815953
292.705816	7999.896602	11.057728	-0.059810	4.815953
292.452796	7999.877034	11.062733	-0.059763	4.815948
292.392572	7999.849226	11.067738	-0.059752	4.815941
292.480334	7999.898929	11.072743	-0.059768	4.815955
292.512348	7999.872803	11.077747	-0.059774	4.815947
292.271806	7999.873769	11.082752	-0.059729	4.815948
292.506792	7999.858825	11.087757	-0.059773	4.815943
292.440251	7999.884339	11.092762	-0.059761	4.815951
292.463015	7999.881557	11.097767	-0.059765	4.815950
292.597328	7999.842334	11.102771	-0.059790	4.815937
292.625484	7999.870644	11.107776	-0.059796	4.815946
292.621812	7999.890892	11.112781	-0.059795	4.815951
292.554477	7999.873642	11.117786	-0.059783	4.815947
292.839544	7999.906637	11.122791	-0.059836	4.815955
292.549729	7999.860748	11.127795	-0.059782	4.815943
292.648703	7999.880730	11.132800	-0.059800	4.815948
292.677410	7999.894088	11.137805	-0.059806	4.815952
292.522822	7999.865627	11.142810	-0.059777	4.815945
292.654766	7999.904380	11.147815	-0.059802	4.815955
292.720065	7999.897030	11.152819	-0.059814	4.815953
292.647787	7999.899995	11.157824	-0.059801	4.815954
292.545503	7999.883176	11.162829	-0.059782	4.815950
292.442025	7999.855648	11.167834	-0.059763	4.815942
292.653861	7999.890514	11.172839	-0.059802	4.815951
292.442778	7999.895223	11.177843	-0.059763	4.815954
292.390548	7999.881454	11.182848	-0.059753	4.815950
292.555665	7999.873787	11.187853	-0.059784	4.815947
292.643250	7999.868980	11.192858	-0.059800	4.815945
292.487079	7999.888585	11.197863	-0.059771	4.815951
292.462981	7999.846473	11.202867	-0.059767	4.815939
292.750192	7999.873095	11.207872	-0.059821	4.815946
292.749162	7999.901941	11.212877	-0.059821	4.815954
292.705289	7999.873362	11.217882	-0.059812	4.815946
292.817211	7999.928850	11.222887	-0.059833	4.815961
292.505682	7999.881496	11.227891	-0.059775	4.815949
292.654733	7999.913079	11.232896	-0.059803	4.815958
292.660903	7999.920682	11.237901	-0.059805	4.815960
292.702539	7999.855187	11.242906	-0.059812	4.815941
292.659403	7999.877922	11.247911	-0.059804	4.815947
292.763096	7999.844553	11.252915	-0.059824	4.815937
292.840318	7999.881240	11.257920	-0.059838	4.815947
292.684099	7999.869849	11.262925	-0.059809	4.815945
292.457306	7999.842209	11.267930	-0.059767	4.815938
292.901750	7999.879180	11.272935	-0.059850	4.815946
292.644351	7999.868082	11.277939	-0.059802	4.815945
292.779510	7999.968882	11.282944	-0.059828	4.815973
292.562941	7999.894402	11.287949	-0.059787	4.815953
292.712698	7999.858667	11.292954	-0.059815	4.815941
292.730701	7999.898548	11.297959	-0.059819	4.815953
292.663465	7999.860993	11.302963	-0.059806	4.815942
292.841919	7999.874944	11.307968	-0.059840	4.815946
292.658395	7999.850231	11.312973	-0.059805	4.815939
292.589152	7999.824396	11.317978	-0.059793	4.815932
292.716560	7999.901541	11.322983	-0.059816	4.815954
292.721139	7999.869571	11.327987	-0.059817	4.815945
292.660994	7999.886651	11.332992	-0.059806	4.815950
292.528502	7999.892794	11.337997	-0.059782	4.815952
292.650240	7999.868304	11.343002	-0.059804	4.815945
292.822100	7999.872516	11.348007	-0.059837	4.815945
292.542079	7999.850318	11.353011	-0.059784	4.815940
292.774973	7999.849230	11.358016	-0.059828	4.815938
292.756058	7999.913020	11.363021	-0.059825	4.815957
292.676846	7999.876315	11.368026	-0.059810	4.815947
293.038197	7999.910702	11.373031	-0.059877	4.815955
292.948203	7999.878075	11.378035	-0.059861	4.815946
292.868961	7999.887327	11.383040	-0.059846	4.815949
292.796862	7999.883883	11.388045	-0.059833	4.815948
292.788662	7999.880536	11.393050	-0.059831	4.815947
292.817518	7999.903515	11.398055	-0.059837	4.815954
292.574741	7999.861689	11.403059	-0.059791	4.815943
292.563486	7999.877524	11.408064	-0.059789	4.815948
292.742195	7999.893617	11.413069	-0.059823	4.815951
292.407756	7999.842639	11.418074	-0.059761	4.815938
292.492737	7999.878398	11.423079	-0.059777	4.815948
292.680958	7999.863671	11.428083	-0.059812	4.815943
292.723624	7999.878351	11.433088	-0.059820	4.815947
292.735216	7999.871090	11.438093	-0.059822	4.815945
292.729882	7999.864589	11.443098	-0.059821	4.815943
292.670531	7999.894510	11.448103	-0.059810	4.815952
292.468707	7999.836331	11.453107	-0.059773	4.815936
292.627307	7999.871295	11.458112	-0.059802	4.815946
292.790451	7999.873211	11.463117	-0.059833	4.815945
292.662973	7999.876238	11.468122	-0.059809	4.815947
292.650110	7999.895250	11.473127	-0.059807	4.815952
292.748308	7999.874606	11.478131	-0.059825	4.815946
292.747735	7999.885292	11.483136	-0.059825	4.815949
292.482002	7999.897554	11.488141	-0.059776	4.815954
292.560302	7999.873341	11.493146	-0.059790	4.815946
292.767135	7999.900635	11.498151	-0.059829	4.815953
292.428134	7999.843161	11.503155	-0.059766	4.815938
292.831557	7999.885796	11.508160	-0.059841	4.815949
292.949430	7999.872992	11.513165	-0.059863	4.815944
292.883376	7999.871796	11.518170	-0.059851	4.815944
292.885279	7999.900697	11.523175	-0.059851	4.815953
292.895412	7999.913715	11.528179	-0.059853	4.815956
292.934732	7999.903754	11.533184	-0.059861	4.815953
292.964636	7999.919271	11.538189	-0.059867	4.815958
292.825692	7999.867582	11.543194	-0.059841	4.815943
292.763391	7999.901724	11.548199	-0.059829	4.815954
292.746800	7999.892880	11.553203	-0.059826	4.815951
292.698271	7999.877041	11.558208	-0.059817	4.815947
292.739649	7999.870323	11.563213	-0.059825	4.815945
292.762671	7999.853652	11.568218	-0.059829	4.815940
292.749261	7999.886547	11.573223	-0.059827	4.815949
292.884027	7999.882602	11.578227	-0.059852	4.815947
292.974056	7999.883184	11.583232	-0.059869	4.815947
292.868182	7999.873780	11.588237	-0.059849	4.815945
292.770269	7999.865591	11.593242	-0.059831	4.815943
292.987902	7999.898426	11.598247	-0.059872	4.815951
292.755237	7999.849303	11.603251	-0.059829	4.815938
292.807046	7999.856669	11.608256	-0.059838	4.815940
292.763345	7999.876187	11.613261	-0.059830	4.815946
292.761476	7999.860131	11.618266	-0.059830	4.815941
292.818916	7999.875081	11.623271	-0.059841	4.815946
292.972558	7999.859723	11.628275	-0.059870	4.815940
292.953202	7999.892511	11.633280	-0.059866	4.815950
292.907244	7999.920538	11.638285	-0.059858	4.815958
292.752166	7999.874968	11.643290	-0.059829	4.815946
292.906426	7999.885272	11.648295	-0.059858	4.815948
292.927056	7999.893138	11.653299	-0.059862	4.815950
292.952859	7999.897893	11.658304	-0.059866	4.815951
293.098930	7999.949729	11.663309	-0.059894	4.815966
292.889767	7999.922410	11.668314	-0.059855	4.815959
292.743562	7999.901583	11.673319	-0.059828	4.815954
292.805497	7999.859971	11.678323	-0.059839	4.815941
292.820260	7999.852768	11.683328	-0.059842	4.815939
292.861694	7999.859945	11.688333	-0.059850	4.815941
292.970633	7999.839497	11.693338	-0.059870	4.815934
292.992521	7999.869830	11.698343	-0.059875	4.815943
292.840935	7999.941887	11.703347	-0.059846	4.815965
292.839714	7999.868129	11.708352	-0.059846	4.815943
292.895773	7999.873436	11.713357	-0.059857	4.815945
292.959430	7999.863918	11.718362	-0.059869	4.815941
293.082306	7999.903575	11.723367	-0.059892	4.815952
293.134324	7999.873538	11.728371	-0.059902	4.815943
293.113889	7999.892412	11.733376	-0.059898	4.815949
293.073088	7999.876714	11.738381	-0.059890	4.815945
293.034249	7999.847158	11.743386	-0.059883	4.815936
293.258876	7999.887602	11.748391	-0.059925	4.815947
293.042502	7999.899696	11.753395	-0.059885	4.815951
292.833077	7999.902297	11.758400	-0.059846	4.815953
292.993410	7999.906299	11.763405	-0.059876	4.815954
292.902174	7999.876856	11.768410	-0.059859	4.815946
292.881350	7999.894654	11.773415	-0.059855	4.815951
292.831279	7999.892680	11.778419	-0.059846	4.815951
292.929583	7999.879520	11.783424	-0.059864	4.815946
292.950022	7999.867076	11.788429	-0.059868	4.815942
292.778639	7999.861822	11.793434	-0.059836	4.815942
293.155574	7999.912525	11.798439	-0.059907	4.815955
293.044989	7999.872041	11.803443	-0.059886	4.815943
292.812833	7999.872091	11.808448	-0.059843	4.815945
292.802570	7999.911456	11.813453	-0.059841	4.815956
292.938009	7999.887217	11.818458	-0.059867	4.815948
292.940781	7999.892620	11.823463	-0.059867	4.815950
292.890404	7999.866059	11.828467	-0.059858	4.815942
292.920165	7999.877299	11.833472	-0.059864	4.815946
292.842914	7999.879105	11.838477	-0.059849	4.815946
292.823954	7999.880905	11.843482	-0.059846	4.815947
292.937332	7999.917183	11.848487	-0.059867	4.815957
293.147319	7999.873996	11.853491	-0.059906	4.815943
292.954477	7999.876900	11.858496	-0.059870	4.815945
293.081810	7999.893126	11.863501	-0.059894	4.815949
293.099873	7999.871020	11.868506	-0.059898	4.815943
293.127981	7999.920705	11.873511	-0.059903	4.815957
293.087562	7999.915701	11.878515	-0.059896	4.815956
293.259081	7999.912426	11.883520	-0.059928	4.815954
293.238112	7999.949460	11.888525	-0.059924	4.815965
293.036935	7999.900910	11.893530	-0.059886	4.815952
293.132447	7999.906936	11.898535	-0.059904	4.815953
293.227607	7999.901200	11.903539	-0.059922	4.815951
292.964482	7999.879308	11.908544	-0.059873	4.815946
292.912653	7999.878372	11.913549	-0.059864	4.815946
293.167152	7999.872335	11.918554	-0.059911	4.815943
293.131093	7999.901612	11.923559	-0.059904	4.815951
292.952928	7999.925090	11.928563	-0.059871	4.815959
292.882353	7999.905642	11.933568	-0.059858	4.815954
293.034453	7999.904151	11.938573	-0.059887	4.815953
292.909580	7999.889056	11.943578	-0.059864	4.815949
292.995729	7999.920562	11.948583	-0.059880	4.815958
293.073625	7999.907029	11.953587	-0.059894	4.815953
292.792721	7999.882676	11.958592	-0.059842	4.815948
292.806817	7999.908592	11.963597	-0.059845	4.815955
293.221273	7999.860586	11.968602	-0.059922	4.815939
293.226530	7999.926954	11.973607	-0.059923	4.815958
292.973802	7999.921284	11.978611	-0.059876	4.815958
293.106397	7999.908749	11.983616	-0.059901	4.815954
293.296696	7999.929330	11.988621	-0.059936	4.815959
292.905574	7999.890140	11.993626	-0.059864	4.815949
293.079987	7999.921119	11.998631	-0.059896	4.815957
293.189540	7999.964808	12.003635	-0.059917	4.815970
292.933990	7999.904579	12.008640	-0.059869	4.815953
292.959912	7999.949949	12.013645	-0.059874	4.815966
293.041959	7999.880916	12.018650	-0.059890	4.815946
293.168031	7999.928113	12.023655	-0.059913	4.815959
293.093639	7999.936383	12.028659	-0.059899	4.815962
293.069529	7999.927402	12.033664	-0.059895	4.815959
293.207783	7999.952378	12.038669	-0.059921	4.815966
293.178969	7999.895216	12.043674	-0.059916	4.815949
293.247221	7999.942427	12.048679	-0.059928	4.815963
293.150348	7999.928912	12.053683	-0.059910	4.815959
292.984747	7999.895974	12.058688	-0.059880	4.815951
293.257482	7999.926609	12.063693	-0.059931	4.815958
293.230121	7999.873749	12.068698	-0.059925	4.815943
293.103152	7999.896023	12.073703	-0.059902	4.815950
293.066774	7999.888956	12.078707	-0.059895	4.815948
293.059861	7999.884563	12.083712	-0.059894	4.815947
293.288673	7999.904778	12.088717	-0.059937	4.815951
293.200972	7999.882880	12.093722	-0.059921	4.815946
293.075770	7999.894499	12.098727	-0.059897	4.815950
293.160256	7999.906737	12.103731	-0.059913	4.815953
293.190438	7999.917984	12.108736	-0.059919	4.815956
293.081574	7999.947001	12.113741	-0.059899	4.815965
293.053090	7999.885571	12.118746	-0.059893	4.815947
293.220986	7999.906811	12.123751	-0.059925	4.815952
293.085451	7999.861597	12.128755	-0.059900	4.815940
293.060907	7999.886808	12.133760	-0.059895	4.815947
293.067347	7999.884797	12.138765	-0.059896	4.815947
293.036879	7999.866081	12.143770	-0.059891	4.815941
293.188990	7999.906272	12.148775	-0.059919	4.815952
293.092978	7999.931248	12.153779	-0.059902	4.815960
292.968891	7999.886243	12.158784	-0.059878	4.815948
293.215250	7999.907846	12.163789	-0.059924	4.815953
293.175206	7999.870786	12.168794	-0.059917	4.815942
293.354539	7999.917886	12.173799	-0.059951	4.815955
293.229078	7999.913469	12.178803	-0.059927	4.815954
293.212555	7999.892869	12.183808	-0.059924	4.815948
293.406858	7999.922074	12.188813	-0.059961	4.815956
293.297306	7999.863439	12.193818	-0.059940	4.815939
293.183371	7999.896639	12.198823	-0.059919	4.815950
293.463843	7999.880389	12.203827	-0.059971	4.815943
293.470447	7999.898687	12.208832	-0.059973	4.815949
293.010492	7999.907405	12.213837	-0.059887	4.815954
293.119413	7999.892301	12.218842	-0.059908	4.815949
293.288567	7999.928528	12.223847	-0.059939	4.815958
293.175157	7999.886923	12.228851	-0.059918	4.815947
293.027840	7999.876763	12.233856	-0.059891	4.815945
293.218004	7999.898410	12.238861	-0.059926	4.815950
293.390123	7999.881252	12.243866	-0.059958	4.815944
293.206090	7999.919586	12.248871	-0.059924	4.815956
293.364859	7999.869052	12.253875	-0.059954	4.815941
293.363140	7999.870099	12.258880	-0.059954	4.815941
293.388696	7999.907981	12.263885	-0.059959	4.815952
293.293757	7999.873126	12.268890	-0.059941	4.815942
293.354237	7999.910576	12.273895	-0.059952	4.815953
293.469231	7999.904133	12.278899	-0.059974	4.815950
293.401280	7999.883664	12.283904	-0.059961	4.815945
293.521813	7999.881597	12.288909	-0.059984	4.815943
293.437859	7999.874730	12.293914	-0.059968	4.815942
293.395980	7999.904969	12.298919	-0.059961	4.815951
293.506095	7999.893093	12.303923	-0.059981	4.815947
293.473187	7999.882882	12.308928	-0.059975	4.815944
293.447008	7999.956159	12.313933	-0.059970	4.815966
293.260535	7999.868333	12.318938	-0.059936	4.815941
293.403886	7999.904089	12.323943	-0.059962	4.815951
293.290202	7999.933018	12.328947	-0.059941	4.815960
292.998471	7999.918086	12.333952	-0.059887	4.815957
293.260317	7999.923940	12.338957	-0.059936	4.815957
293.208251	7999.885592	12.343962	-0.059926	4.815946
293.418826	7999.899062	12.348967	-0.059966	4.815949
293.257805	7999.874757	12.353971	-0.059936	4.815943
293.232154	7999.909568	12.358976	-0.059931	4.815953
293.326603	7999.897406	12.363981	-0.059949	4.815949
293.410266	7999.852983	12.368986	-0.059964	4.815936
293.461760	7999.905233	12.373991	-0.059974	4.815951
293.427651	7999.886450	12.378995	-0.059968	4.815945
293.280113	7999.879492	12.384000	-0.059940	4.815944
293.433456	7999.904743	12.389005	-0.059969	4.815951
293.305926	7999.892806	12.394010	-0.059945	4.815948
293.349482	7999.907504	12.399015	-0.059954	4.815952
293.225327	7999.889216	12.404019	-0.059931	4.815947
293.165590	7999.909510	12.409024	-0.059920	4.815953
293.235123	7999.942851	12.414029	-0.059933	4.815963
293.165307	7999.893491	12.419034	-0.059920	4.815949
293.270220	7999.923202	12.424039	-0.059939	4.815957
293.263085	7999.914531	12.429043	-0.059938	4.815954
293.160850	7999.883818	12.434048	-0.059919	4.815946
293.105184	7999.923424	12.439053	-0.059909	4.815958
293.215853	7999.888045	12.444058	-0.059930	4.815947
293.268327	7999.914662	12.449063	-0.059939	4.815954
293.389549	7999.917951	12.454067	-0.059962	4.815955
293.208858	7999.892219	12.459072	-0.059929	4.815948
293.407712	7999.893718	12.464077	-0.059966	4.815947
293.137013	7999.850313	12.469082	-0.059915	4.815936
293.207488	7999.906114	12.474087	-0.059929	4.815952
293.406986	7999.850980	12.479091	-0.059966	4.815935
293.095458	7999.863475	12.484096	-0.059908	4.815940
293.332836	7999.913772	12.489101	-0.059952	4.815954
293.414048	7999.888543	12.494106	-0.059967	4.815946
293.278419	7999.892490	12.499111	-0.059942	4.815948
293.202159	7999.880420	12.504115	-0.059928	4.815945
293.453129	7999.894626	12.509120	-0.059975	4.815947
293.456575	7999.894698	12.514125	-0.059976	4.815947
293.158074	7999.867885	12.519130	-0.059920	4.815941
293.242373	7999.903633	12.524135	-0.059936	4.815951
293.353816	7999.916363	12.529139	-0.059957	4.815954
293.282579	7999.899040	12.534144	-0.059944	4.815950
293.402251	7999.895889	12.539149	-0.059966	4.815948
293.251432	7999.868564	12.544154	-0.059938	4.815941
293.257786	7999.861207	12.549159	-0.059939	4.815939
293.428137	7999.877149	12.554163	-0.059971	4.815942
293.313204	7999.888955	12.559168	-0.059950	4.815946
293.575566	7999.881994	12.564173	-0.059999	4.815943
293.252174	7999.863278	12.569178	-0.059939	4.815939
293.356896	7999.880160	12.574183	-0.059958	4.815944
293.620546	7999.887117	12.579187	-0.060007	4.815944
293.368487	7999.862220	12.584192	-0.059961	4.815938
293.273819	7999.915009	12.589197	-0.059943	4.815954
293.469604	7999.835225	12.594202	-0.059980	4.815930
293.540008	7999.881407	12.599207	-0.059993	4.815943
293.520865	7999.890686	12.604211	-0.059989	4.815946
293.214198	7999.876550	12.609216	-0.059932	4.815943
293.421083	7999.911327	12.614221	-0.059971	4.815952
293.279227	7999.868135	12.619226	-0.059945	4.815941
293.202136	7999.898800	12.624231	-0.059930	4.815950
293.230476	7999.859782	12.629235	-0.059936	4.815938
293.244954	7999.881430	12.634240	-0.059938	4.815945
293.442532	7999.925657	12.639245	-0.059975	4.815956
293.447758	7999.873391	12.644250	-0.059976	4.815941
293.517930	7999.903537	12.649255	-0.059990	4.815950
293.482264	7999.872970	12.654259	-0.059983	4.815941
293.428470	7999.894441	12.659264	-0.059973	4.815947
293.398039	7999.880001	12.664269	-0.059967	4.815943
293.316469	7999.865696	12.669274	-0.059952	4.815940
293.476945	7999.896421	12.674279	-0.059982	4.815948
293.547809	7999.856040	12.679283	-0.059996	4.815936
293.318176	7999.868960	12.684288	-0.059953	4.815941
293.276076	7999.894920	12.689293	-0.059945	4.815948
293.205022	7999.862638	12.694298	-0.059932	4.815939
293.574959	7999.936730	12.699303	-0.060001	4.815959
293.607243	7999.893507	12.704307	-0.060007	4.815946
293.526904	7999.879225	12.709312	-0.059992	4.815942
293.699745	7999.902694	12.714317	-0.060025	4.815948
293.561410	7999.848878	12.719322	-0.059999	4.815933
293.303379	7999.868761	12.724327	-0.059951	4.815941
293.536031	7999.899734	12.729331	-0.059994	4.815948
293.635913	7999.869502	12.734336	-0.060013	4.815939
293.567524	7999.899257	12.739341	-0.060000	4.815948
293.613797	7999.863772	12.744346	-0.060009	4.815937
293.675822	7999.976066	12.749351	-0.060021	4.815970
293.423375	7999.882760	12.754355	-0.059974	4.815944
293.428482	7999.864692	12.759360	-0.059975	4.815939
293.583191	7999.911344	12.764365	-0.060004	4.815951
293.456749	7999.865226	12.769370	-0.059980	4.815939
293.468537	7999.877206	12.774375	-0.059983	4.815942
293.590930	7999.860210	12.779379	-0.060005	4.815936
293.520171	7999.855722	12.784384	-0.059992	4.815936
293.478884	7999.881697	12.789389	-0.059985	4.815943
293.380619	7999.839299	12.794394	-0.059967	4.815931
293.643404	7999.876166	12.799399	-0.060016	4.815941
293.345951	7999.849372	12.804403	-0.059960	4.815935
293.435310	7999.861699	12.809408	-0.059977	4.815938
293.488709	7999.893677	12.814413	-0.059987	4.815947
293.443358	7999.838350	12.819418	-0.059979	4.815931
293.311894	7999.857336	12.824423	-0.059954	4.815937
293.407518	7999.868709	12.829427	-0.059972	4.815940
293.434387	7999.868139	12.834432	-0.059977	4.815940
293.446174	7999.872638	12.839437	-0.059980	4.815941
293.406455	7999.847340	12.844442	-0.059972	4.815934
293.613452	7999.872501	12.849447	-0.060011	4.815940
293.523596	7999.860183	12.854451	-0.059994	4.815937
293.625721	7999.870605	12.859456	-0.060013	4.815939
293.443900	7999.883328	12.864461	-0.059980	4.815944
293.506430	7999.873790	12.869466	-0.059991	4.815941
293.403091	7999.889014	12.874471	-0.059972	4.815946
293.607846	7999.851076	12.879475	-0.060010	4.815934
293.527810	7999.877413	12.884480	-0.059996	4.815942
293.479966	7999.882962	12.889485	-0.059987	4.815944
293.321704	7999.864051	12.894490	-0.059957	4.815939
293.395401	7999.957320	12.899495	-0.059971	4.815966
293.399666	7999.865491	12.904499	-0.059972	4.815939
293.316951	7999.849028	12.909504	-0.059957	4.815935
293.550399	7999.869328	12.914509	-0.060000	4.815939
293.433883	7999.846904	12.919514	-0.059979	4.815933
293.412277	7999.871101	12.924519	-0.059975	4.815941
293.494518	7999.858716	12.929523	-0.059990	4.815936
293.702589	7999.853971	12.934528	-0.060029	4.815934
293.809747	7999.855935	12.939533	-0.060049	4.815934
293.709330	7999.837011	12.944538	-0.060030	4.815929
293.679229	7999.878153	12.949543	-0.060025	4.815941
293.544401	7999.877839	12.954547	-0.060000	4.815942
293.451952	7999.850511	12.959552	-0.059983	4.815934
293.591957	7999.861624	12.964557	-0.060009	4.815937
293.471282	7999.844469	12.969562	-0.059987	4.815932
293.589675	7999.982373	12.974567	-0.060009	4.815972
293.545128	7999.884310	12.979571	-0.060001	4.815944
293.485335	7999.868265	12.984576	-0.059990	4.815939
293.689817	7999.908343	12.989581	-0.060028	4.815950
293.483532	7999.852218	12.994586	-0.059989	4.815935
293.561073	7999.865398	12.999591	-0.060004	4.815938
293.541559	7999.875738	13.004595	-0.060000	4.815941
293.539926	7999.867167	13.009600	-0.060000	4.815939
293.458176	7999.881716	13.014605	-0.059985	4.815943
293.772206	7999.881042	13.019610	-0.060044	4.815941
293.508550	7999.883722	13.024615	-0.059995	4.815944
293.513406	7999.877406	13.029619	-0.059996	4.815942
293.645264	7999.843483	13.034624	-0.060020	4.815931
293.806245	7999.894524	13.039629	-0.060050	4.815945
293.452989	7999.860299	13.044634	-0.059985	4.815937
293.385236	7999.880447	13.049639	-0.059972	4.815943
293.433414	7999.877060	13.054643	-0.059981	4.815942
293.540557	7999.868336	13.059648	-0.060001	4.815939
293.454440	7999.888149	13.064653	-0.059985	4.815945
293.517386	7999.857243	13.069658	-0.059997	4.815936
293.495533	7999.862197	13.074663	-0.059993	4.815937
293.657614	7999.853406	13.079667	-0.060023	4.815934
293.634627	7999.875440	13.084672	-0.060019	4.815941
293.728106	7999.893187	13.089677	-0.060037	4.815945
293.604487	7999.849257	13.094682	-0.060014	4.815933
293.567631	7999.874244	13.099687	-0.060007	4.815941
293.552589	7999.864360	13.104691	-0.060004	4.815938
293.359496	7999.849089	13.109696	-0.059968	4.815934
293.544289	7999.893083	13.114701	-0.060003	4.815946
293.495753	7999.849455	13.119706	-0.059994	4.815934
293.536810	7999.964573	13.124711	-0.060002	4.815967
293.530061	7999.868268	13.129715	-0.060000	4.815939
293.413260	7999.867214	13.134720	-0.059979	4.815939
293.727547	7999.882577	13.139725	-0.060037	4.815942
293.571436	7999.870118	13.144730	-0.060008	4.815939
293.649284	7999.892923	13.149735	-0.060023	4.815946
293.620511	7999.883857	13.154739	-0.060018	4.815943
293.463873	7999.872457	13.159744	-0.059989	4.815941
293.641462	7999.886394	13.164749	-0.060022	4.815944
293.526016	7999.865058	13.169754	-0.060000	4.815938
293.546007	7999.883601	13.174759	-0.060004	4.815943
293.610861	7999.876243	13.179763	-0.060016	4.815941
293.569656	7999.878707	13.184768	-0.060009	4.815942
293.506637	7999.901079	13.189773	-0.059997	4.815949
293.436245	7999.889115	13.194778	-0.059984	4.815946
293.413681	7999.880162	13.199783	-0.059980	4.815943
293.646722	7999.867323	13.204787	-0.060024	4.815938
293.389200	7999.861564	13.209792	-0.059976	4.815938
293.268671	7999.877543	13.214797	-0.059953	4.815943
293.349479	7999.833069	13.219802	-0.059968	4.815930
293.567629	7999.883015	13.224807	-0.060009	4.815943
293.483948	7999.880429	13.229811	-0.059994	4.815943
293.457701	7999.898128	13.234816	-0.059989	4.815948
293.592867	7999.914497	13.239821	-0.060014	4.815952
293.697260	7999.875797	13.244826	-0.060034	4.815940
293.598145	7999.896442	13.249831	-0.060015	4.815947
293.675806	7999.882905	13.254835	-0.060030	4.815942
293.441726	7999.863680	13.259840	-0.059986	4.815938
293.482259	7999.889010	13.264845	-0.059994	4.815945
293.601381	7999.870885	13.269850	-0.060016	4.815939
293.534679	7999.875021	13.274855	-0.060004	4.815941
293.382633	7999.846605	13.279859	-0.059976	4.815933
293.406343	7999.827809	13.284864	-0.059980	4.815928
293.546311	7999.879535	13.289869	-0.060006	4.815942
293.469025	7999.913403	13.294874	-0.059992	4.815952
293.475760	7999.856890	13.299879	-0.059993	4.815936
293.761445	7999.870661	13.304883	-0.060047	4.815938
293.689549	7999.861877	13.309888	-0.060033	4.815936
293.688298	7999.886445	13.314893	-0.060033	4.815943
293.664289	7999.923423	13.319898	-0.060029	4.815954
293.608710	7999.893561	13.324903	-0.060019	4.815946
293.737147	7999.908738	13.329907	-0.060043	4.815950
293.577402	7999.886594	13.334912	-0.060013	4.815944
293.656387	7999.876288	13.339917	-0.060028	4.815941
293.548033	7999.849738	13.344922	-0.060008	4.815933
293.460872	7999.883426	13.349927	-0.059992	4.815944
293.895683	7999.880681	13.354931	-0.060073	4.815941
293.643640	7999.866471	13.359936	-0.060026	4.815938
293.554461	7999.900123	13.364941	-0.060009	4.815948
293.494084	7999.886205	13.369946	-0.059998	4.815944
293.580064	7999.928396	13.374951	-0.060014	4.815956
293.677170	7999.920558	13.379955	-0.060032	4.815953
293.477513	7999.872035	13.384960	-0.059995	4.815940
293.739980	7999.909965	13.389965	-0.060044	4.815950
293.651250	7999.890185	13.394970	-0.060028	4.815945
293.626905	7999.903644	13.399975	-0.060023	4.815949
293.761872	7999.924285	13.404979	-0.060049	4.815954
293.800275	7999.891862	13.409984	-0.060056	4.815944
293.685993	7999.912230	13.414989	-0.060035	4.815951
293.609228	7999.879844	13.419994	-0.060020	4.815942
293.585826	7999.878357	13.424999	-0.060016	4.815941
293.707332	7999.912646	13.430003	-0.060039	4.815951
293.391047	7999.854514	13.435008	-0.059980	4.815936
293.568607	7999.906926	13.440013	-0.060013	4.815950
293.545440	7999.860555	13.445018	-0.060009	4.815936
293.466602	7999.851644	13.450023	-0.059994	4.815934
293.589351	7999.867786	13.455027	-0.060017	4.815938
293.542225	7999.847697	13.460032	-0.060009	4.815933
293.494269	7999.870344	13.465037	-0.060000	4.815940
293.432508	7999.862813	13.470042	-0.059988	4.815938
293.477104	7999.947001	13.475047	-0.059997	4.815962
293.659836	7999.869116	13.480051	-0.060031	4.815938
293.627557	7999.866399	13.485056	-0.060025	4.815938
293.590113	7999.909544	13.490061	-0.060018	4.815951
293.557332	7999.885442	13.495066	-0.060012	4.815944
293.465354	7999.903011	13.500071	-0.059995	4.815949
293.755679	7999.900836	13.505075	-0.060049	4.815947
293.817154	7999.885934	13.510080	-0.060061	4.815942
293.738690	7999.927263	13.515085	-0.060046	4.815955
293.733435	7999.883355	13.520090	-0.060045	4.815942
293.614486	7999.867300	13.525095	-0.060023	4.815938
293.815974	7999.887017	13.530099	-0.060061	4.815943
293.568295	7999.876094	13.535104	-0.060015	4.815941
293.563705	7999.903807	13.540109	-0.060014	4.815949
293.504499	7999.869603	13.545114	-0.060003	4.815939
293.531713	7999.882934	13.550119	-0.060008	4.815943
293.509033	7999.884667	13.555123	-0.060004	4.815944
293.512620	7999.844127	13.560128	-0.060005	4.815932
293.513502	7999.880491	13.565133	-0.060005	4.815942
293.377379	7999.853434	13.570138	-0.059980	4.815935
293.441107	7999.875981	13.575143	-0.059992	4.815941
293.685914	7999.884732	13.580147	-0.060038	4.815943
293.519923	7999.850717	13.585152	-0.060007	4.815934
293.402231	7999.879573	13.590157	-0.059985	4.815943
293.544208	7999.851178	13.595162	-0.060011	4.815934
293.581099	7999.853998	13.600167	-0.060018	4.815934
293.593171	7999.874534	13.605171	-0.060021	4.815940
293.653321	7999.886328	13.610176	-0.060032	4.815943
293.728789	7999.908021	13.615181	-0.060046	4.815949
293.677472	7999.857929	13.620186	-0.060037	4.815935
293.619467	7999.892149	13.625191	-0.060026	4.815945
293.604987	7999.894031	13.630195	-0.060023	4.815946
293.634273	7999.846479	13.635200	-0.060029	4.815932
293.739313	7999.899707	13.640205	-0.060049	4.815947
293.585713	7999.858436	13.645210	-0.060020	4.815936
293.642668	7999.870172	13.650215	-0.060031	4.815939
293.590737	7999.860683	13.655219	-0.060021	4.815936
293.582903	7999.842380	13.660224	-0.060020	4.815931
293.992337	7999.874442	13.665229	-0.060096	4.815938
293.592530	7999.869293	13.670234	-0.060022	4.815939
293.702042	7999.887332	13.675239	-0.060042	4.815943
293.896479	7999.878063	13.680243	-0.060079	4.815940
293.809827	7999.871147	13.685248	-0.060063	4.815938
293.853578	7999.905086	13.690253	-0.060071	4.815948
293.637664	7999.860541	13.695258	-0.060031	4.815936
293.554791	7999.866520	13.700263	-0.060015	4.815938
293.539749	7999.894042	13.705267	-0.060013	4.815946
293.568733	7999.865723	13.710272	-0.060018	4.815938
293.526839	7999.900237	13.715277	-0.060010	4.815948
293.508613	7999.872125	13.720282	-0.060007	4.815940
293.550017	7999.872889	13.725287	-0.060015	4.815940
293.885733	7999.903606	13.730291	-0.060078	4.815947
293.624885	7999.882823	13.735296	-0.060029	4.815942
293.565091	7999.941593	13.740301	-0.060018	4.815960
293.703944	7999.915278	13.745306	-0.060044	4.815951
293.566376	7999.881782	13.750311	-0.060018	4.815942
293.583227	7999.921644	13.755315	-0.060022	4.815954
293.556845	7999.865594	13.760320	-0.060017	4.815938
293.800073	7999.898899	13.765325	-0.060062	4.815946
293.710591	7999.876968	13.770330	-0.060046	4.815940
293.691062	7999.876620	13.775335	-0.060042	4.815940
293.587588	7999.915355	13.780339	-0.060023	4.815952
293.595023	7999.868473	13.785344	-0.060024	4.815938
293.574030	7999.896956	13.790349	-0.060021	4.815947
293.611116	7999.874128	13.795354	-0.060028	4.815940
293.521810	7999.884264	13.800359	-0.060011	4.815943
293.525409	7999.900370	13.805363	-0.060012	4.815948
293.518383	7999.853224	13.810368	-0.060011	4.815934
293.686149	7999.889427	13.815373	-0.060042	4.815944
293.699037	7999.864020	13.820378	-0.060044	4.815936
293.760485	7999.879044	13.825383	-0.060056	4.815941
293.866461	7999.919463	13.830387	-0.060076	4.815952
293.704482	7999.862008	13.835392	-0.060046	4.815936
293.745116	7999.903372	13.840397	-0.060053	4.815948
293.901254	7999.900886	13.845402	-0.060082	4.815946
293.758499	7999.912184	13.850407	-0.060056	4.815950
293.794418	7999.901092	13.855411	-0.060063	4.815947
293.640863	7999.891886	13.860416	-0.060034	4.815945
293.806320	7999.959042	13.865421	-0.060065	4.815964
293.842009	7999.893437	13.870426	-0.060072	4.815944
293.652097	7999.875017	13.875431	-0.060037	4.815940
293.729754	7999.907438	13.880435	-0.060051	4.815949
293.606658	7999.863518	13.885440	-0.060028	4.815937
293.651255	7999.895335	13.890445	-0.060037	4.815946
293.581357	7999.876968	13.895450	-0.060024	4.815941
293.495139	7999.858303	13.900455	-0.060008	4.815936
293.727461	7999.908509	13.905459	-0.060051	4.815949
293.628399	7999.884265	13.910464	-0.060033	4.815943
293.713836	7999.894384	13.915469	-0.060049	4.815945
293.672549	7999.860507	13.920474	-0.060041	4.815936
293.652930	7999.878327	13.925479	-0.060038	4.815941
293.826800	7999.907159	13.930483	-0.060070	4.815948
293.739938	7999.877795	13.935488	-0.060054	4.815940
293.688266	7999.906787	13.940493	-0.060045	4.815949
293.789107	7999.917186	13.945498	-0.060063	4.815951
293.820743	7999.916703	13.950503	-0.060069	4.815951
293.877578	7999.910268	13.955507	-0.060080	4.815949
293.816759	7999.872828	13.960512	-0.060069	4.815938
293.955716	7999.883923	13.965517	-0.060095	4.815941
293.980377	7999.892932	13.970522	-0.060099	4.815943
293.827874	7999.890158	13.975527	-0.060071	4.815943
293.780007	7999.902119	13.980531	-0.060062	4.815947
293.657788	7999.899897	13.985536	-0.060040	4.815947
293.880278	7999.907172	13.990541	-0.060081	4.815948
293.822199	7999.880470	13.995546	-0.060070	4.815941
293.704687	7999.887954	14.000551	-0.060049	4.815943
293.816527	7999.907104	14.005555	-0.060070	4.815948
293.638744	7999.866461	14.010560	-0.060037	4.815937
293.712000	7999.876357	14.015565	-0.060050	4.815940
293.738517	7999.901432	14.020570	-0.060055	4.815947
293.535626	7999.908427	14.025575	-0.060018	4.815950
293.838664	7999.919309	14.030579	-0.060074	4.815952
293.809764	7999.886727	14.035584	-0.060069	4.815942
293.812083	7999.939149	14.040589	-0.060069	4.815958
293.791600	7999.904583	14.045594	-0.060066	4.815948
293.808087	7999.898480	14.050599	-0.060069	4.815946
293.873619	7999.914647	14.055603	-0.060081	4.815950
293.636018	7999.876119	14.060608	-0.060037	4.815940
293.807013	7999.880317	14.065613	-0.060069	4.815941
293.948650	7999.881842	14.070618	-0.060095	4.815940
293.738795	7999.880159	14.075623	-0.060056	4.815941
293.862539	7999.888838	14.080627	-0.060079	4.815943
293.692330	7999.869709	14.085632	-0.060048	4.815938
293.911363	7999.929292	14.090637	-0.060089	4.815954
293.872905	7999.910430	14.095642	-0.060082	4.815949
293.624331	7999.900559	14.100647	-0.060036	4.815947
293.812991	7999.947831	14.105651	-0.060071	4.815960
293.707062	7999.887123	14.110656	-0.060051	4.815943
293.810986	7999.944605	14.115661	-0.060071	4.815959
293.836680	7999.890575	14.120666	-0.060075	4.815943
293.803649	7999.900669	14.125671	-0.060069	4.815946
293.766882	7999.914970	14.130675	-0.060063	4.815951
293.872360	7999.888046	14.135680	-0.060082	4.815942
293.705482	7999.882872	14.140685	-0.060051	4.815942
293.657616	7999.887351	14.145690	-0.060043	4.815943
293.887284	7999.902239	14.150695	-0.060085	4.815946
293.972726	7999.941215	14.155699	-0.060101	4.815957
293.819530	7999.889264	14.160704	-0.060073	4.815943
293.771896	7999.909779	14.165709	-0.060064	4.815949
293.893256	7999.895971	14.170714	-0.060087	4.815945
293.847571	7999.890871	14.175719	-0.060078	4.815943
293.823065	7999.897914	14.180723	-0.060074	4.815946
293.931937	7999.874258	14.185728	-0.060094	4.815938
294.007655	7999.921607	14.190733	-0.060109	4.815951
293.742993	7999.882585	14.195738	-0.060059	4.815941
293.761131	7999.869030	14.200743	-0.060063	4.815937
294.126521	7999.894946	14.205747	-0.060131	4.815943
293.732368	7999.876005	14.210752	-0.060058	4.815940
293.737584	7999.916723	14.215757	-0.060059	4.815951
293.797902	7999.887906	14.220762	-0.060070	4.815943
293.804656	7999.885901	14.225767	-0.060071	4.815942
293.866834	7999.894526	14.230771	-0.060083	4.815944
294.022340	7999.885616	14.235776	-0.060112	4.815941
293.929232	7999.926677	14.240781	-0.060095	4.815953
293.708797	7999.908769	14.245786	-0.060054	4.815949
293.808347	7999.898838	14.250791	-0.060072	4.815946
294.078718	7999.916606	14.255795	-0.060123	4.815950
293.864854	7999.638034	14.260800	-0.060083	4.815869

293.747234	7996.412794	14.265805	-0.060059	4.814928
293.695017	7990.818884	14.270810	-0.060046	4.813293
293.602538	7984.011025	14.275815	-0.060024	4.811304
293.582924	7976.714217	14.280819	-0.060016	4.809170
293.520749	7969.040140	14.285824	-0.059999	4.806925
293.640335	7961.194757	14.290829	-0.060017	4.804628
293.610957	7953.379316	14.295834	-0.060006	4.802339
293.599516	7945.394289	14.300839	-0.059999	4.799999
293.680193	7937.475398	14.305843	-0.060009	4.797677
293.457947	7929.389296	14.310848	-0.059962	4.795307
293.313228	7921.398965	14.315853	-0.059930	4.792963
293.332445	7913.397178	14.320858	-0.059929	4.790614
293.251468	7905.391345	14.325863	-0.059909	4.788262
292.986257	7897.424819	14.330867	-0.059854	4.785922
293.056959	7889.429305	14.335872	-0.059862	4.783571
293.166211	7881.392671	14.340877	-0.059877	4.781207
292.953473	7873.456908	14.345882	-0.059833	4.778872
293.130650	7865.369828	14.350887	-0.059860	4.776490
293.103298	7857.394947	14.355891	-0.059850	4.774141
292.796721	7849.338403	14.360896	-0.059788	4.771767
292.743185	7841.381713	14.365901	-0.059773	4.769421
292.891014	7833.401144	14.370906	-0.059795	4.767066
292.955786	7825.363040	14.375911	-0.059802	4.764693
292.941110	7817.486354	14.380915	-0.059794	4.762367
292.779190	7809.350618	14.385920	-0.059759	4.759963
292.873667	7801.441045	14.390925	-0.059772	4.757625
292.870501	7793.382086	14.395930	-0.059766	4.755241
292.712972	7785.338881	14.400935	-0.059731	4.752861
292.674724	7777.310790	14.405939	-0.059719	4.750485
292.475423	7769.345820	14.410944	-0.059677	4.748126
292.367184	7761.314412	14.415949	-0.059652	4.745746
292.543285	7753.385293	14.420954	-0.059679	4.743394
292.417190	7745.320693	14.425959	-0.059651	4.741002
292.391889	7737.336073	14.430963	-0.059641	4.738632
292.408170	7729.334929	14.435968	-0.059639	4.736256
292.322223	7721.349240	14.440973	-0.059618	4.733884
292.304846	7713.301168	14.445978	-0.059609	4.731491
291.896253	7705.282243	14.450983	-0.059528	4.729108
291.974517	7697.311622	14.455987	-0.059538	4.726736
291.943307	7689.286153	14.460992	-0.059527	4.724346
291.874757	7681.352391	14.465997	-0.059509	4.721983
291.969676	7673.361476	14.471002	-0.059521	4.719601
291.955291	7665.349390	14.476007	-0.059513	4.717213
291.970682	7657.347949	14.481011	-0.059511	4.714825
291.677800	7649.285880	14.486016	-0.059452	4.712420
291.839750	7641.267901	14.491021	-0.059477	4.710025
291.773194	7633.325992	14.496026	-0.059459	4.707652
291.598064	7625.288987	14.501031	-0.059421	4.705250
291.650993	7617.363593	14.506035	-0.059426	4.702880
291.529208	7609.310282	14.511040	-0.059398	4.700470
291.394514	7601.329851	14.516045	-0.059368	4.698081
291.706202	7593.322867	14.521050	-0.059421	4.695682
291.596599	7585.269578	14.526055	-0.059395	4.693269
291.615145	7577.279788	14.531059	-0.059394	4.690873
291.496365	7569.296140	14.536064	-0.059366	4.688478
291.472976	7561.251836	14.541069	-0.059357	4.686063
291.464296	7553.301182	14.546074	-0.059350	4.683676
291.204936	7545.280091	14.551079	-0.059297	4.681266
291.503048	7537.379240	14.556083	-0.059347	4.678890
291.406943	7529.286621	14.561088	-0.059324	4.676456
291.177979	7521.226431	14.566093	-0.059276	4.674031
290.977856	7513.189364	14.571098	-0.059234	4.671612
291.187475	7505.197408	14.576103	-0.059268	4.669204
291.182089	7497.211324	14.581107	-0.059262	4.666797
290.937821	7489.256972	14.586112	-0.059211	4.664398
290.988215	7481.240184	14.591117	-0.059215	4.661979
290.793207	7473.238631	14.596122	-0.059174	4.659564
290.708402	7465.256350	14.601127	-0.059153	4.657153
290.754411	7457.257207	14.606131	-0.059157	4.654736
290.702063	7449.237995	14.611136	-0.059142	4.652311
290.615912	7441.190852	14.616141	-0.059121	4.649877
290.668064	7433.270259	14.621146	-0.059125	4.647480
290.584245	7425.200626	14.626151	-0.059104	4.645036
290.668153	7417.271934	14.631155	-0.059115	4.642634
290.667041	7409.187407	14.636160	-0.059110	4.640183
290.504418	7401.259905	14.641165	-0.059074	4.637779
290.373188	7393.232811	14.646170	-0.059045	4.635343
290.349677	7385.208289	14.651175	-0.059035	4.632907
290.314920	7377.163314	14.656179	-0.059023	4.630463
290.368401	7369.222467	14.661184	-0.059028	4.628049
290.187878	7361.161968	14.666189	-0.058990	4.625598
290.298468	7353.252198	14.671194	-0.059005	4.623191
290.279752	7345.175001	14.676199	-0.058996	4.620732
290.286425	7337.246657	14.681203	-0.058993	4.618317
289.855118	7329.197723	14.686208	-0.058907	4.615865
289.987637	7321.167491	14.691213	-0.058927	4.613416
290.067272	7313.172095	14.696218	-0.058936	4.610977
289.951932	7305.178612	14.701223	-0.058910	4.608537
290.041836	7297.145692	14.706227	-0.058921	4.606084
290.046115	7289.145550	14.711232	-0.058917	4.603639
289.993724	7281.176168	14.716237	-0.058902	4.601203
289.850525	7273.207930	14.721242	-0.058870	4.598766
289.726997	7265.196054	14.726247	-0.058842	4.596314
289.948961	7257.172239	14.731251	-0.058878	4.593857
289.674152	7249.103783	14.736256	-0.058822	4.591385
289.753855	7241.103833	14.741261	-0.058832	4.588932
289.773012	7233.141748	14.746266	-0.058830	4.586490
289.451366	7225.124126	14.751271	-0.058765	4.584030
289.458380	7217.158434	14.756275	-0.058761	4.581584
289.463018	7209.160427	14.761280	-0.058757	4.579127
289.598132	7201.152339	14.766285	-0.058777	4.576666
289.486065	7193.151920	14.771290	-0.058751	4.574205
289.316342	7185.097120	14.776295	-0.058715	4.571727
289.361067	7177.098071	14.781299	-0.058718	4.569264
289.187780	7169.110863	14.786304	-0.058680	4.566803
289.101748	7161.157209	14.791309	-0.058659	4.564352
289.105623	7153.197528	14.796314	-0.058655	4.561898
289.159803	7145.131742	14.801319	-0.058660	4.559409
289.197806	7137.196774	14.806323	-0.058662	4.556959
289.074216	7129.150345	14.811328	-0.058634	4.554474
289.161352	7121.092538	14.816333	-0.058645	4.551984
288.945795	7113.071439	14.821338	-0.058599	4.549504
288.779815	7105.084894	14.826343	-0.058563	4.547032
288.920307	7097.119747	14.831347	-0.058584	4.544567
288.822143	7089.136652	14.836352	-0.058561	4.542094
288.757295	7081.118531	14.841357	-0.058544	4.539610
288.807546	7073.194925	14.846362	-0.058548	4.537153
288.653069	7065.125625	14.851367	-0.058514	4.534649
288.560965	7057.139989	14.856371	-0.058492	4.532170
288.539758	7049.070981	14.861376	-0.058483	4.529664
288.437694	7041.109324	14.866381	-0.058459	4.527190
288.419716	7033.068295	14.871386	-0.058450	4.524690
288.335261	7025.135437	14.876391	-0.058429	4.522222
288.631098	7017.128552	14.881395	-0.058479	4.519731
288.478311	7009.182762	14.886400	-0.058446	4.517256
288.269641	7001.117534	14.891405	-0.058402	4.514742
288.324271	6993.028190	14.896410	-0.058407	4.512220
288.340569	6985.014642	14.901415	-0.058405	4.509720
288.154916	6977.079898	14.906419	-0.058365	4.507243
288.111776	6969.034676	14.911424	-0.058352	4.504731
288.162018	6961.121156	14.916429	-0.058356	4.502258
288.127744	6953.087801	14.921434	-0.058345	4.499747
288.195458	6945.100093	14.926439	-0.058352	4.497248
288.043314	6937.082602	14.931443	-0.058319	4.494738
287.761962	6929.049749	14.936448	-0.058261	4.492222
287.724186	6921.006595	14.941453	-0.058249	4.489702
287.810941	6913.072471	14.946458	-0.058260	4.487214
287.858373	6905.018684	14.951463	-0.058264	4.484688
287.956164	6897.105220	14.956467	-0.058277	4.482204
287.616059	6889.099622	14.961472	-0.058208	4.479689
287.724612	6881.105517	14.966477	-0.058223	4.477178
287.541638	6873.034185	14.971482	-0.058184	4.474639
287.499053	6864.980075	14.976487	-0.058171	4.472106
287.888334	6856.989842	14.981491	-0.058238	4.469592
287.636690	6849.046946	14.986496	-0.058187	4.467090
287.303232	6841.028212	14.991501	-0.058119	4.464562
287.339651	6833.119258	14.996506	-0.058121	4.462068
287.206167	6825.040390	15.001511	-0.058091	4.459519
287.220408	6817.075373	15.006515	-0.058089	4.457005
287.101464	6809.026369	15.011520	-0.058061	4.454462
287.039552	6801.000152	15.016525	-0.058045	4.451926
287.243474	6793.033795	15.021530	-0.058077	4.449407
287.001796	6785.020734	15.026535	-0.058027	4.446871
287.083501	6777.040141	15.031539	-0.058037	4.444345
287.025998	6769.034173	15.036544	-0.058022	4.441809
286.960700	6761.039796	15.041549	-0.058004	4.439276
287.056641	6753.078561	15.046554	-0.058017	4.436751
286.894834	6745.000093	15.051559	-0.057982	4.434188
286.869669	6736.954143	15.056563	-0.057972	4.431633
286.725332	6728.974311	15.061568	-0.057940	4.429098
286.671684	6720.959637	15.066573	-0.057925	4.426550
286.617044	6712.974156	15.071578	-0.057910	4.424011
286.532878	6704.966221	15.076583	-0.057889	4.421462
286.502233	6697.011233	15.081587	-0.057878	4.418929
286.395576	6688.984474	15.086592	-0.057853	4.416372
286.324595	6680.997167	15.091597	-0.057835	4.413825
286.304390	6672.933542	15.096602	-0.057826	4.411253
286.241459	6664.974029	15.101607	-0.057809	4.408713
286.173267	6657.005529	15.106611	-0.057791	4.406168
286.113818	6649.001487	15.111616	-0.057775	4.403611
286.227888	6640.995628	15.116621	-0.057791	4.401052
286.258416	6633.048343	15.121626	-0.057792	4.398510
285.958667	6624.994665	15.126631	-0.057731	4.395931
286.083487	6617.008446	15.131635	-0.057749	4.393374
286.201357	6608.942203	15.136640	-0.057766	4.390790
286.111010	6600.941417	15.141645	-0.057744	4.388224
286.133790	6592.962017	15.146650	-0.057743	4.385665
286.076822	6584.990520	15.151655	-0.057727	4.383105
285.990723	6576.988235	15.156659	-0.057706	4.380535
285.649180	6569.041572	15.161664	-0.057637	4.377979
285.873942	6560.952301	15.166669	-0.057674	4.375379
285.816968	6552.959873	15.171674	-0.057658	4.372807
285.478075	6544.929549	15.176679	-0.057590	4.370220
285.644168	6537.015435	15.181683	-0.057616	4.367672
285.537264	6528.969336	15.186688	-0.057591	4.365077
285.745530	6521.026952	15.191693	-0.057624	4.362517
285.565897	6513.004283	15.196698	-0.057586	4.359927
285.503603	6505.042314	15.201703	-0.057569	4.357356
285.567992	6496.993866	15.206707	-0.057576	4.354756
285.376089	6488.891271	15.211712	-0.057535	4.352135
285.371546	6480.911679	15.216717	-0.057529	4.349554
285.506273	6472.954432	15.221722	-0.057549	4.346979
285.398679	6464.903399	15.226727	-0.057524	4.344371
285.390368	6456.974749	15.231731	-0.057517	4.341802
285.217885	6448.945259	15.236736	-0.057480	4.339197
285.259195	6440.963565	15.241741	-0.057483	4.336608
284.983065	6432.958375	15.246746	-0.057426	4.334007
285.068315	6424.922940	15.251751	-0.057437	4.331397
285.071360	6416.945851	15.256755	-0.057432	4.328804
284.938089	6408.933174	15.261760	-0.057402	4.326198
285.114062	6400.988007	15.266765	-0.057430	4.323613
285.036831	6392.959871	15.271770	-0.057410	4.320998
284.858752	6384.964634	15.276775	-0.057372	4.318392
284.839581	6376.994838	15.281779	-0.057363	4.315794
284.957250	6368.963759	15.286784	-0.057380	4.313175
284.882123	6360.888172	15.291789	-0.057361	4.310538
284.693230	6352.966267	15.296794	-0.057321	4.307949
284.665252	6344.855597	15.301799	-0.057310	4.305299
284.806757	6336.975208	15.306803	-0.057332	4.302723
284.578281	6328.947591	15.311808	-0.057284	4.300094
284.608754	6320.941015	15.316813	-0.057285	4.297473
284.529163	6312.928508	15.321818	-0.057265	4.294847
284.196947	6304.906796	15.326823	-0.057198	4.292215
284.128233	6296.915394	15.331827	-0.057180	4.289593
284.093409	6288.964250	15.336832	-0.057168	4.286983
284.021095	6280.893419	15.341837	-0.057149	4.284332
283.995792	6272.984150	15.346842	-0.057140	4.281733
284.057749	6264.882073	15.351847	-0.057146	4.279069
284.265009	6256.957921	15.356851	-0.057180	4.276463
283.801812	6248.895698	15.361856	-0.057088	4.273805
283.766495	6240.838536	15.366861	-0.057076	4.271151
283.899759	6232.894873	15.371866	-0.057096	4.268533
283.706544	6224.890428	15.376871	-0.057055	4.265891
283.743682	6216.918297	15.381875	-0.057057	4.263260
283.617050	6208.894773	15.386880	-0.057028	4.260610
283.571501	6200.909162	15.391885	-0.057015	4.257970
283.560245	6192.916316	15.396890	-0.057007	4.255327
283.455812	6184.882771	15.401895	-0.056983	4.252668
283.545490	6176.869940	15.406899	-0.056994	4.250016
283.443938	6168.918958	15.411904	-0.056970	4.247381
283.520815	6160.858047	15.416909	-0.056979	4.244710
283.526880	6152.983801	15.421914	-0.056976	4.242098
283.186550	6144.945120	15.426919	-0.056907	4.239426
283.213149	6136.982469	15.431923	-0.056907	4.236782
283.216859	6128.927745	15.436928	-0.056902	4.234105
283.247993	6120.874548	15.441933	-0.056903	4.231428
283.366220	6112.915937	15.446938	-0.056920	4.228780
282.975248	6104.892180	15.451943	-0.056842	4.226105
283.066601	6096.909705	15.456947	-0.056854	4.223447
283.142723	6088.929852	15.461952	-0.056863	4.220787
282.966220	6080.933231	15.466957	-0.056825	4.218118
282.954710	6072.952893	15.471962	-0.056818	4.215454
282.886225	6064.903580	15.476967	-0.056800	4.212764
282.809606	6056.910104	15.481971	-0.056780	4.210092
282.844163	6048.949269	15.486976	-0.056782	4.207430
282.873638	6040.898493	15.491981	-0.056782	4.204736
282.729397	6032.995981	15.496986	-0.056750	4.202088
282.680704	6024.898194	15.501991	-0.056736	4.199374
282.735487	6016.997084	15.506995	-0.056741	4.196725
282.641962	6008.856157	15.512000	-0.056718	4.193993
282.607927	6000.807074	15.517005	-0.056707	4.191290
282.724974	5992.870965	15.522010	-0.056724	4.188625
282.683377	5984.841725	15.527015	-0.056711	4.185926
282.738135	5976.910251	15.532019	-0.056716	4.183258
282.366465	5968.918377	15.537024	-0.056642	4.180564
282.324882	5960.944567	15.542029	-0.056629	4.177878
282.387670	5952.927222	15.547034	-0.056635	4.175177
282.209274	5944.880183	15.552039	-0.056597	4.172461
282.304506	5936.904580	15.557043	-0.056610	4.169770
282.067644	5928.922648	15.562048	-0.056560	4.167072
281.909365	5920.899102	15.567053	-0.056526	4.164359
282.158082	5912.933996	15.572058	-0.056567	4.161669
282.031727	5904.883906	15.577063	-0.056538	4.158943
282.082571	5896.918090	15.582067	-0.056543	4.156247
281.975844	5888.896352	15.587072	-0.056518	4.153528
281.863677	5880.857086	15.592077	-0.056492	4.150801
281.938192	5872.909783	15.597082	-0.056500	4.148106
281.751129	5864.861566	15.602087	-0.056460	4.145372
281.738823	5856.899151	15.607091	-0.056453	4.142667
281.787200	5848.882023	15.612096	-0.056457	4.139942
281.622875	5840.924290	15.617101	-0.056421	4.137234
281.698681	5832.907584	15.622106	-0.056430	4.134506
281.505788	5824.870692	15.627111	-0.056389	4.131766
281.587740	5816.857052	15.632115	-0.056399	4.129036
281.372191	5808.878394	15.637120	-0.056354	4.126313
281.287973	5800.900444	15.642125	-0.056333	4.123589
281.314581	5792.912889	15.647130	-0.056333	4.120862
281.288876	5784.901442	15.652135	-0.056323	4.118124
281.200768	5776.919494	15.657139	-0.056302	4.115393
281.374860	5768.890519	15.662144	-0.056329	4.112648
281.192733	5760.794138	15.667149	-0.056290	4.109873
281.206809	5752.869185	15.672154	-0.056287	4.107158
281.150952	5744.834626	15.677159	-0.056272	4.104403
281.114309	5736.916668	15.682163	-0.056260	4.101686
280.911735	5728.913796	15.687168	-0.056217	4.098935
280.931070	5720.930795	15.692173	-0.056215	4.096193
280.957907	5712.900205	15.697178	-0.056215	4.093433
281.005931	5704.864249	15.702183	-0.056219	4.090669
281.004310	5696.925349	15.707187	-0.056214	4.087936
281.017628	5688.895161	15.712192	-0.056211	4.085170
281.022568	5680.930491	15.717197	-0.056207	4.082424
280.898779	5672.940863	15.722202	-0.056179	4.079666
280.756125	5664.959236	15.727207	-0.056147	4.076909
280.850606	5656.928659	15.732211	-0.056160	4.074137
280.674649	5648.903273	15.737216	-0.056122	4.071360
280.535744	5640.913563	15.742221	-0.056091	4.068595
280.437681	5632.931342	15.747226	-0.056067	4.065831
280.337279	5624.943878	15.752231	-0.056043	4.063063
280.599928	5616.935699	15.757235	-0.056087	4.060291
280.436069	5608.964403	15.762240	-0.056052	4.057524
280.287498	5600.914378	15.767245	-0.056019	4.054728
280.255746	5592.961389	15.772250	-0.056008	4.051965
280.288153	5584.918741	15.777255	-0.056009	4.049170
280.323184	5576.927296	15.782259	-0.056010	4.046391
280.242438	5568.945198	15.787264	-0.055990	4.043612
280.221816	5560.918650	15.792269	-0.055981	4.040816
280.224491	5552.979987	15.797274	-0.055976	4.038050
280.173852	5544.906710	15.802279	-0.055962	4.035233
280.172594	5536.856702	15.807283	-0.055956	4.032424
279.923588	5528.870995	15.812288	-0.055905	4.029631
279.803877	5520.876539	15.817293	-0.055877	4.026835
279.931024	5512.921823	15.822298	-0.055896	4.024055
279.730458	5504.899153	15.827303	-0.055854	4.021244
279.724262	5496.927318	15.832307	-0.055847	4.018452
279.649785	5488.928353	15.837312	-0.055828	4.015648
279.517546	5480.912598	15.842317	-0.055799	4.012835
279.593202	5472.908609	15.847322	-0.055808	4.010027
279.265601	5464.908255	15.852327	-0.055741	4.007212
279.356657	5456.913070	15.857331	-0.055753	4.004403
279.423402	5448.910336	15.862336	-0.055761	4.001590
279.175069	5440.927148	15.867341	-0.055709	3.998776
279.312887	5432.947596	15.872346	-0.055730	3.995968
279.372169	5424.906268	15.877351	-0.055736	3.993135
279.487193	5416.867245	15.882355	-0.055752	3.990301
279.147448	5408.908304	15.887360	-0.055684	3.987487
279.360209	5400.871832	15.892365	-0.055718	3.984652
279.433327	5392.941817	15.897370	-0.055727	3.981850
279.191949	5384.917879	15.902375	-0.055676	3.979008
279.171897	5376.960183	15.907379	-0.055668	3.976191
278.939566	5368.971207	15.912384	-0.055619	3.973358
278.988129	5360.916071	15.917389	-0.055623	3.970503
278.966726	5352.970259	15.922394	-0.055614	3.967684
278.843950	5344.908227	15.927399	-0.055586	3.964820
278.960894	5337.001643	15.932403	-0.055603	3.962014
278.889350	5328.995341	15.937408	-0.055584	3.959166
278.681762	5321.003006	15.942413	-0.055541	3.956320
278.786078	5312.969310	15.947418	-0.055555	3.953462
278.559887	5304.917684	15.952423	-0.055508	3.950589
278.641038	5296.960635	15.957427	-0.055518	3.947754
278.601975	5288.940685	15.962432	-0.055505	3.944892
278.463484	5280.982065	15.967437	-0.055474	3.942048
278.753786	5272.984942	15.972442	-0.055523	3.939196
278.436023	5264.988092	15.977447	-0.055459	3.936331
278.563885	5256.956302	15.982451	-0.055478	3.933460
278.525201	5248.962882	15.987456	-0.055465	3.930597
278.144038	5241.003454	15.992461	-0.055389	3.927738
278.255297	5232.999597	15.997466	-0.055405	3.924870
278.077182	5225.029792	16.002471	-0.055366	3.922007
278.235780	5216.981369	16.007475	-0.055391	3.919119
278.051941	5209.000193	16.012480	-0.055352	3.916247
278.284955	5200.978041	16.017485	-0.055390	3.913366
277.916849	5192.985864	16.022490	-0.055316	3.910483
277.832808	5184.964611	16.027495	-0.055295	3.907593
277.878129	5176.982606	16.032499	-0.055299	3.904716
277.900909	5169.003291	16.037504	-0.055298	3.901838
277.616904	5161.002302	16.042509	-0.055240	3.898945
277.778483	5153.007861	16.047514	-0.055265	3.896060
277.791273	5144.963920	16.052519	-0.055262	3.893152
277.730816	5136.963415	16.057523	-0.055246	3.890256
277.696289	5129.009791	16.062528	-0.055234	3.887376
277.605650	5120.987486	16.067533	-0.055212	3.884468
277.419244	5113.020992	16.072538	-0.055172	3.881575
277.306457	5105.009361	16.077543	-0.055146	3.878666
277.412909	5097.001711	16.082547	-0.055161	3.875760
277.356243	5088.824020	16.087552	-0.055145	3.872787
277.245832	5080.821953	16.092557	-0.055119	3.869874
277.325406	5072.888734	16.097562	-0.055129	3.866988
277.215875	5064.926958	16.102567	-0.055104	3.864086
277.271122	5056.960672	16.107571	-0.055109	3.861183
277.156398	5048.993250	16.112576	-0.055082	3.858275
277.198417	5040.951622	16.117581	-0.055085	3.855340
277.116673	5032.985170	16.122586	-0.055065	3.852427
276.806603	5024.983429	16.127591	-0.055002	3.849496
276.994033	5016.976120	16.132595	-0.055032	3.846569
276.880024	5008.969185	16.137600	-0.055005	3.843635
276.639473	5001.030731	16.142605	-0.054955	3.840721
276.675444	4993.055074	16.147610	-0.054957	3.837796
276.710482	4985.024320	16.152615	-0.054958	3.834850
276.565128	4977.050534	16.157619	-0.054926	3.831918
276.739647	4968.981887	16.162624	-0.054953	3.828955
276.512107	4961.001293	16.167629	-0.054906	3.826015
276.503018	4953.055362	16.172634	-0.054899	3.823089
276.458105	4945.030300	16.177639	-0.054886	3.820131
276.490303	4937.062133	16.182643	-0.054887	3.817194
276.515770	4929.048886	16.187648	-0.054886	3.814237
276.445376	4921.065896	16.192653	-0.054868	3.811288
276.501783	4913.059926	16.197658	-0.054873	3.808330
276.470102	4905.056770	16.202663	-0.054862	3.805369
276.169432	4897.109055	16.207667	-0.054801	3.802420
276.072745	4889.107853	16.212672	-0.054778	3.799454
276.229471	4881.078073	16.217677	-0.054802	3.796480
276.207797	4873.090120	16.222682	-0.054793	3.793516
275.920708	4865.012124	16.227687	-0.054734	3.790510
275.969936	4857.081388	16.232691	-0.054738	3.787564
275.996383	4849.049901	16.237696	-0.054738	3.784578
276.037715	4841.121969	16.242701	-0.054741	3.781628
275.890723	4833.099913	16.247706	-0.054708	3.778636
275.961082	4825.082280	16.252711	-0.054716	3.775649
275.853327	4817.084905	16.257715	-0.054691	3.772662
275.834010	4809.089476	16.262720	-0.054682	3.769677
275.846996	4801.109320	16.267725	-0.054680	3.766695
275.828660	4793.103151	16.272730	-0.054671	3.763700
275.633976	4785.121497	16.277735	-0.054630	3.760708
275.758054	4777.115357	16.282739	-0.054648	3.757712
275.704064	4769.123854	16.287744	-0.054633	3.754715
275.468178	4761.102414	16.292749	-0.054584	3.751700
275.515805	4753.082698	16.297754	-0.054587	3.748690
275.313502	4745.084710	16.302759	-0.054545	3.745680
275.325429	4737.107472	16.307763	-0.054542	3.742680
275.142416	4729.144496	16.312768	-0.054502	3.739678
275.035020	4721.149360	16.317773	-0.054477	3.736664
275.234205	4713.121854	16.322778	-0.054509	3.733642
274.978745	4705.124080	16.327783	-0.054457	3.730618
274.969272	4697.153097	16.332787	-0.054450	3.727608
275.025283	4689.155564	16.337792	-0.054455	3.724587
274.925369	4681.185842	16.342797	-0.054431	3.721570
275.034856	4673.209445	16.347802	-0.054447	3.718553
274.846507	4665.161917	16.352807	-0.054406	3.715500
274.804359	4657.110183	16.357811	-0.054393	3.712446
274.673104	4649.112704	16.362816	-0.054364	3.709408
274.734852	4641.093102	16.367821	-0.054370	3.706364
274.671076	4633.165271	16.372826	-0.054353	3.703349
274.307454	4625.201639	16.377831	-0.054280	3.700311
274.338290	4617.203760	16.382835	-0.054281	3.697266
274.581488	4609.191384	16.387840	-0.054321	3.694219
274.429596	4601.169359	16.392845	-0.054288	3.691156
274.306688	4593.227406	16.397850	-0.054260	3.688122
274.419968	4585.192521	16.402855	-0.054276	3.685056
274.289824	4577.252013	16.407859	-0.054246	3.682017
274.150179	4569.233924	16.412864	-0.054215	3.678945
274.152546	4561.233640	16.417869	-0.054211	3.675882
274.369268	4553.240561	16.422874	-0.054246	3.672824
274.329287	4545.161186	16.427879	-0.054233	3.669723
274.322820	4537.199429	16.432883	-0.054227	3.666667
274.434219	4529.208056	16.437888	-0.054243	3.663599
274.084294	4521.245981	16.442893	-0.054172	3.660528
274.214601	4513.271605	16.447898	-0.054191	3.657462
274.244890	4505.257912	16.452903	-0.054192	3.654376
274.051269	4497.227189	16.457907	-0.054151	3.651275
273.936053	4489.257941	16.462912	-0.054124	3.648197
273.966072	4481.201609	16.467917	-0.054125	3.645087
273.872907	4473.287265	16.472922	-0.054102	3.642025
273.727135	4465.260583	16.477927	-0.054070	3.638916
273.667758	4457.296192	16.482931	-0.054054	3.635831
273.658018	4449.244196	16.487936	-0.054047	3.632711
273.373338	4441.234091	16.492941	-0.053989	3.629597
273.436494	4433.253681	16.497946	-0.053995	3.626501
273.354836	4425.269979	16.502951	-0.053975	3.623397
273.435568	4417.275499	16.507955	-0.053985	3.620290
273.412422	4409.303881	16.512960	-0.053975	3.617187
273.315297	4401.285783	16.517965	-0.053952	3.614062
273.485077	4393.291262	16.522970	-0.053979	3.610950
273.239062	4385.327068	16.527975	-0.053928	3.607835
273.088263	4377.307248	16.532979	-0.053895	3.604699
273.252339	4369.370519	16.537984	-0.053920	3.601602
273.100501	4361.347978	16.542989	-0.053887	3.598459
273.053152	4353.360193	16.547994	-0.053873	3.595330
273.018753	4345.325116	16.552999	-0.053861	3.592180
272.931512	4337.357358	16.558003	-0.053840	3.589053
272.969357	4329.347917	16.563008	-0.053842	3.585909
272.786301	4321.389886	16.568013	-0.053803	3.582778
272.787794	4313.392333	16.573018	-0.053798	3.579632
272.650001	4305.436412	16.578023	-0.053767	3.576497
272.685486	4297.405328	16.583027	-0.053768	3.573334
272.656975	4289.379642	16.588032	-0.053758	3.570169
272.647434	4281.420602	16.593037	-0.053751	3.567027
272.469547	4273.430266	16.598042	-0.053713	3.563866
272.576996	4265.422351	16.603047	-0.053728	3.560703
272.618812	4257.431039	16.608051	-0.053730	3.557542
272.434464	4249.400364	16.613056	-0.053691	3.554356
272.180844	4241.311226	16.618061	-0.053639	3.551142
272.467566	4233.348574	16.623066	-0.053687	3.547991
272.389211	4225.356988	16.628071	-0.053667	3.544815
272.312618	4217.438421	16.633075	-0.053648	3.541665
272.218451	4209.443532	16.638080	-0.053625	3.538482
272.222108	4201.403931	16.643085	-0.053621	3.535280
271.969217	4193.458108	16.648090	-0.053569	3.532106
271.836347	4185.420606	16.653095	-0.053539	3.528895
272.100208	4177.402903	16.658099	-0.053583	3.525702
271.979311	4169.477527	16.663104	-0.053555	3.522531
271.798890	4161.455404	16.668109	-0.053516	3.519317
271.967534	4153.500803	16.673114	-0.053543	3.516137
271.758950	4145.486159	16.678119	-0.053499	3.512919
271.730022	4137.459853	16.683123	-0.053488	3.509698
271.736496	4129.491087	16.688128	-0.053484	3.506499
271.879201	4121.462494	16.693133	-0.053506	3.503277
271.681425	4113.541022	16.698138	-0.053464	3.500085
271.597666	4105.536725	16.703143	-0.053443	3.496860
271.537965	4097.522516	16.708147	-0.053427	3.493629
271.497081	4089.543701	16.713152	-0.053414	3.490409
271.155129	4081.571615	16.718157	-0.053345	3.487180
271.324340	4073.575129	16.723162	-0.053372	3.483954
271.366073	4065.577378	16.728167	-0.053374	3.480721
271.303519	4057.607511	16.733171	-0.053358	3.477492
271.348660	4049.594304	16.738176	-0.053361	3.474247
271.278045	4041.554557	16.743181	-0.053343	3.470984
271.118060	4033.569402	16.748186	-0.053308	3.467737
271.045161	4025.553459	16.753191	-0.053289	3.464477
271.146803	4017.602665	16.758195	-0.053303	3.461246
271.007168	4009.619334	16.763200	-0.053272	3.457992
270.979910	4001.602508	16.768205	-0.053261	3.454724
270.883154	3993.628651	16.773210	-0.053238	3.451468
270.781987	3985.605396	16.778215	-0.053214	3.448189
270.714548	3977.623780	16.783219	-0.053197	3.444925
270.561472	3969.693245	16.788224	-0.053163	3.441676
270.460849	3961.671558	16.793229	-0.053139	3.438388
270.644598	3953.652967	16.798234	-0.053168	3.435108
270.377958	3945.653211	16.803239	-0.053114	3.431817
270.438336	3937.643154	16.808243	-0.053120	3.428530
270.377443	3929.647556	16.813248	-0.053103	3.425242
270.241629	3921.695342	16.818253	-0.053073	3.421966
270.289715	3913.694146	16.823258	-0.053077	3.418672
270.488274	3905.680780	16.828263	-0.053108	3.415376
270.229368	3897.701938	16.833267	-0.053055	3.412075
270.114297	3889.721403	16.838272	-0.053029	3.408775
270.046257	3881.716857	16.843277	-0.053011	3.405463
270.165731	3873.783844	16.848282	-0.053028	3.402185
269.815992	3865.783465	16.853287	-0.052958	3.398859
269.861342	3857.777912	16.858291	-0.052961	3.395541
269.878563	3849.717844	16.863296	-0.052959	3.392196
269.737458	3841.705193	16.868301	-0.052928	3.388863
269.775650	3833.731307	16.873306	-0.052930	3.385548
269.802266	3825.763937	16.878311	-0.052930	3.382233
269.709423	3817.779937	16.883315	-0.052907	3.378903
269.735308	3809.811834	16.888320	-0.052907	3.375580
269.563414	3801.800960	16.893325	-0.052870	3.372230
269.630767	3793.819001	16.898330	-0.052877	3.368896
269.348953	3785.813297	16.903335	-0.052820	3.365537
269.438440	3777.869925	16.908339	-0.052831	3.362214
269.459707	3769.881357	16.913344	-0.052830	3.358867
269.189574	3761.876493	16.918349	-0.052775	3.355498
269.310666	3753.847874	16.923354	-0.052792	3.352130
269.328477	3745.843532	16.928359	-0.052790	3.348766
269.247898	3737.843808	16.933363	-0.052770	3.345396
269.108865	3729.905360	16.938368	-0.052739	3.342047
269.285212	3721.883382	16.943373	-0.052767	3.338671
269.296514	3713.912525	16.948378	-0.052764	3.335306
269.116754	3705.896096	16.953383	-0.052725	3.331912
269.124795	3697.891548	16.958387	-0.052722	3.328527
269.009616	3689.904386	16.963392	-0.052695	3.325141
268.918034	3681.934406	16.968397	-0.052673	3.321759
268.890488	3673.984646	16.973402	-0.052663	3.318385
268.702784	3665.985009	16.978407	-0.052623	3.314981
268.636482	3657.940464	16.983411	-0.052605	3.311558
268.657521	3649.927385	16.988416	-0.052604	3.308149
268.586751	3641.939441	16.993421	-0.052586	3.304743
268.611853	3634.030322	16.998426	-0.052585	3.301371
268.499782	3626.038359	17.003431	-0.052559	3.297955
268.689094	3618.009742	17.008435	-0.052589	3.294531
268.726386	3610.008736	17.013440	-0.052591	3.291109
268.553786	3602.034739	17.018445	-0.052554	3.287688
268.394606	3594.081762	17.023450	-0.052519	3.284273
268.201858	3586.100878	17.028455	-0.052478	3.280840
268.176005	3578.131632	17.033459	-0.052468	3.277416
268.181577	3570.106232	17.038464	-0.052464	3.273965
268.134442	3562.072299	17.043469	-0.052450	3.270504
268.212187	3554.100062	17.048474	-0.052460	3.267072
268.054274	3546.106860	17.053479	-0.052425	3.263617
267.829071	3538.124690	17.058483	-0.052378	3.260161
268.054968	3530.175067	17.063488	-0.052415	3.256733
267.835047	3522.143083	17.068493	-0.052369	3.253248
267.809823	3514.143822	17.073498	-0.052359	3.249782
267.946451	3506.152700	17.078503	-0.052379	3.246321
267.954699	3498.171021	17.083507	-0.052376	3.242856
267.698224	3490.223619	17.088512	-0.052323	3.239392
267.641996	3482.227694	17.093517	-0.052307	3.235910
267.665109	3474.190822	17.098522	-0.052306	3.232410
267.624258	3466.157825	17.103527	-0.052294	3.228906
267.428566	3458.187228	17.108531	-0.052252	3.225419
267.633097	3450.241756	17.113536	-0.052285	3.221955
267.392180	3442.235607	17.118541	-0.052235	3.218443
267.220516	3434.263926	17.123546	-0.052198	3.214944
267.246784	3426.276118	17.128551	-0.052198	3.211443
267.440311	3418.255764	17.133555	-0.052229	3.207931
267.180816	3410.325646	17.138560	-0.052175	3.204436
266.955810	3402.339356	17.143565	-0.052128	3.200914
267.007687	3394.362820	17.148570	-0.052133	3.197403
266.944608	3386.340754	17.153575	-0.052116	3.193864
267.088567	3378.298136	17.158579	-0.052138	3.190321
266.946254	3370.361430	17.163584	-0.052106	3.186808
266.867078	3362.349954	17.168589	-0.052086	3.183261
267.031885	3354.376379	17.173594	-0.052112	3.179738
266.664442	3346.441898	17.178599	-0.052038	3.176205
266.749869	3338.400747	17.183603	-0.052049	3.172640
266.728748	3330.411803	17.188608	-0.052040	3.169089
266.538973	3322.419943	17.193613	-0.052000	3.165527
266.874411	3314.446254	17.198618	-0.052057	3.161990
266.752986	3306.477030	17.203623	-0.052029	3.158432
266.409595	3298.519394	17.208627	-0.051960	3.154866
266.374531	3290.509689	17.213632	-0.051949	3.151286
266.197564	3282.458684	17.218637	-0.051910	3.147677
266.373488	3274.505365	17.223642	-0.051938	3.144123
266.219554	3266.505357	17.228647	-0.051904	3.140529
266.365279	3258.527081	17.233651	-0.051926	3.136955
266.197994	3250.554382	17.238656	-0.051890	3.133365
266.135332	3242.525181	17.243661	-0.051873	3.129750
266.187528	3234.554990	17.248666	-0.051878	3.126162
266.126533	3226.588439	17.253671	-0.051861	3.122567
266.000090	3218.608512	17.258675	-0.051833	3.118959
266.141888	3210.636965	17.263680	-0.051854	3.115362
265.975224	3202.614025	17.268685	-0.051818	3.111725
265.872796	3194.658933	17.273690	-0.051794	3.108116
265.864168	3186.641222	17.278695	-0.051787	3.104479
265.892790	3178.654634	17.283699	-0.051787	3.100854
265.663616	3170.714038	17.288704	-0.051739	3.097234
265.551009	3162.688261	17.293709	-0.051713	3.093576
265.540839	3154.691917	17.298714	-0.051706	3.089932
265.417021	3146.755387	17.303719	-0.051678	3.086305
265.324055	3138.746596	17.308723	-0.051656	3.082643
265.490086	3130.760207	17.313728	-0.051682	3.078998
265.629353	3122.740912	17.318733	-0.051702	3.075333
265.560937	3114.694228	17.323738	-0.051684	3.071641
265.328292	3106.742537	17.328743	-0.051636	3.067981
265.386232	3098.747908	17.333747	-0.051642	3.064310
265.416430	3090.812446	17.338752	-0.051642	3.060661
265.011544	3082.856879	17.343757	-0.051562	3.056977
264.916608	3074.879504	17.348762	-0.051539	3.053294
264.873543	3066.842987	17.353767	-0.051526	3.049581
265.073121	3058.867711	17.358771	-0.051558	3.045904
264.962965	3050.927663	17.363776	-0.051532	3.042224
264.686862	3042.944309	17.368781	-0.051476	3.038511
264.759114	3034.962568	17.373786	-0.051484	3.034811
264.683029	3026.921198	17.378791	-0.051465	3.031072
264.745914	3018.935804	17.383795	-0.051471	3.027361
264.733849	3010.979321	17.388800	-0.051464	3.023655
264.444942	3003.001758	17.393805	-0.051405	3.019921
264.395501	2995.050096	17.398810	-0.051391	3.016207
264.647629	2987.001433	17.403815	-0.051433	3.012457
264.466525	2979.024517	17.408819	-0.051394	3.008715
264.347945	2971.051087	17.413824	-0.051367	3.004973
264.353010	2963.088007	17.418829	-0.051362	3.001237
264.354765	2955.127883	17.423834	-0.051358	2.997498
264.287713	2947.110627	17.428839	-0.051340	2.993724
264.099509	2939.096397	17.433843	-0.051300	2.989940
264.063632	2931.131924	17.438848	-0.051288	2.986183
263.806276	2923.159267	17.443853	-0.051235	2.982406
263.944030	2915.168218	17.448858	-0.051256	2.978635
263.899376	2907.173605	17.453863	-0.051242	2.974849
263.880374	2899.185811	17.458867	-0.051234	2.971062
263.784041	2891.240770	17.463872	-0.051210	2.967287
263.626071	2883.248772	17.468877	-0.051176	2.963481
263.665136	2875.280173	17.473882	-0.051178	2.959692
263.608052	2867.318952	17.478887	-0.051162	2.955897
263.619773	2859.295854	17.483891	-0.051159	2.952070
263.756472	2851.299124	17.488896	-0.051180	2.948258
263.386614	2843.320858	17.493901	-0.051106	2.944424
263.593480	2835.359418	17.498906	-0.051139	2.940622
263.469206	2827.388620	17.503911	-0.051111	2.936794
263.355129	2819.393386	17.508915	-0.051085	2.932949
263.298746	2811.419316	17.513920	-0.051069	2.929113
263.139910	2803.420183	17.518925	-0.051034	2.925254
263.257090	2795.476102	17.523930	-0.051051	2.921431
263.097373	2787.496900	17.528935	-0.051016	2.917572
263.230657	2779.442772	17.533939	-0.051036	2.913687
263.153380	2771.420410	17.538944	-0.051016	2.909800
262.970234	2763.465476	17.543949	-0.050977	2.905936
262.893636	2755.518530	17.548954	-0.050958	2.902076
262.793759	2747.545588	17.553959	-0.050934	2.898197
262.892275	2739.522404	17.558963	-0.050947	2.894299
262.770285	2731.572732	17.563968	-0.050919	2.890419
262.696845	2723.599013	17.568973	-0.050901	2.886526
262.799547	2715.622337	17.573978	-0.050915	2.882635
262.611778	2707.663721	17.578983	-0.050875	2.878732
262.793624	2699.664738	17.583987	-0.050903	2.874823
262.613149	2691.680609	17.588992	-0.050865	2.870897
262.652171	2683.671589	17.593997	-0.050867	2.866966
262.545470	2675.732312	17.599002	-0.050842	2.863055
262.590337	2667.737570	17.604007	-0.050845	2.859120
262.459260	2659.771634	17.609011	-0.050816	2.855184
262.407880	2651.797696	17.614016	-0.050801	2.851244
262.266028	2643.811553	17.619021	-0.050769	2.847286
262.305930	2635.835640	17.624026	-0.050772	2.843338
262.087005	2627.886155	17.629031	-0.050726	2.839384
261.893457	2619.916727	17.634035	-0.050685	2.835415
262.005530	2611.890073	17.639040	-0.050700	2.831429
261.839630	2603.918097	17.644045	-0.050664	2.827450
261.808157	2595.937780	17.649050	-0.050653	2.823468
261.780076	2587.961479	17.654055	-0.050643	2.819483
261.996992	2579.950443	17.659059	-0.050678	2.815488
261.985308	2571.982374	17.664064	-0.050671	2.811497
261.736973	2564.014762	17.669069	-0.050620	2.807486
261.855713	2556.052002	17.674074	-0.050637	2.803494
261.636863	2548.088420	17.679079	-0.050591	2.799475
261.516215	2540.122002	17.684083	-0.050563	2.795456
261.480118	2532.122737	17.689088	-0.050552	2.791418
261.405567	2524.114799	17.694093	-0.050533	2.787368
261.367032	2516.161241	17.699098	-0.050520	2.783342
261.206871	2508.188961	17.704103	-0.050485	2.779294
261.319709	2500.197953	17.709107	-0.050501	2.775246
261.426325	2492.226015	17.714112	-0.050516	2.771201
261.110263	2484.267025	17.719117	-0.050452	2.767132
261.293137	2476.303996	17.724122	-0.050481	2.763085
261.096997	2468.319156	17.729127	-0.050439	2.758998
260.910678	2460.357926	17.734131	-0.050400	2.754917
260.987542	2452.285739	17.739136	-0.050409	2.750790
260.919996	2444.319849	17.744141	-0.050391	2.746702
261.018979	2436.357826	17.749146	-0.050404	2.742620
260.824230	2428.402138	17.754151	-0.050363	2.738517
260.726752	2420.447616	17.759155	-0.050340	2.734415
260.711635	2412.449990	17.764160	-0.050332	2.730289
260.666473	2404.473450	17.769165	-0.050318	2.726166
260.645256	2396.519429	17.774170	-0.050309	2.722050
260.592671	2388.560701	17.779175	-0.050294	2.717923
260.417659	2380.587160	17.784179	-0.050257	2.713775
260.373917	2372.586865	17.789184	-0.050243	2.709615
260.363747	2364.597872	17.794189	-0.050236	2.705456
260.193548	2356.664224	17.799194	-0.050200	2.701310
260.250680	2348.683381	17.804199	-0.050205	2.697146
260.371273	2340.692303	17.809203	-0.050222	2.692975
260.301571	2332.713747	17.814208	-0.050204	2.688793
259.997899	2324.747828	17.819213	-0.050143	2.684595
260.090683	2316.797852	17.824218	-0.050155	2.680424
259.865756	2308.849316	17.829223	-0.050108	2.676228
259.855027	2300.825338	17.834227	-0.050101	2.671998
259.737016	2292.846556	17.839232	-0.050074	2.667779
259.829089	2284.852632	17.844237	-0.050086	2.663559
259.847830	2276.897310	17.849242	-0.050084	2.659348
259.583169	2268.968456	17.854247	-0.050030	2.655126
259.522553	2260.961151	17.859251	-0.050013	2.650868
259.493089	2253.005741	17.864256	-0.050003	2.646633
259.332419	2245.029064	17.869261	-0.049968	2.642372
259.447098	2237.081025	17.874266	-0.049984	2.638137
259.447872	2229.079123	17.879271	-0.049979	2.633859
259.420357	2221.083206	17.884275	-0.049969	2.629575
259.521651	2213.127235	17.889280	-0.049983	2.625314
259.159645	2205.196185	17.894285	-0.049910	2.621030
259.221987	2197.223645	17.899290	-0.049917	2.616743
259.057058	2189.236362	17.904295	-0.049881	2.612427
259.095350	2181.241269	17.909299	-0.049883	2.608113
259.105564	2173.281891	17.914304	-0.049880	2.603809
258.930053	2165.346340	17.919309	-0.049842	2.599498
258.909408	2157.393872	17.924314	-0.049833	2.595182
258.924737	2149.215433	17.929319	-0.049830	2.590738
258.828471	2141.266316	17.934323	-0.049807	2.586403
258.698415	2133.353101	17.939328	-0.049778	2.582079
258.708836	2125.401950	17.944333	-0.049775	2.577736
258.468996	2117.477307	17.949338	-0.049725	2.573383
258.518584	2109.496026	17.954343	-0.049729	2.569012
258.465240	2101.514249	17.959347	-0.049714	2.564626
258.511409	2093.589205	17.964352	-0.049718	2.560270
258.372490	2085.633295	17.969357	-0.049687	2.555877
258.297648	2077.648573	17.974362	-0.049668	2.551465
258.268090	2069.667462	17.979367	-0.049657	2.547050
258.294184	2061.692024	17.984371	-0.049657	2.542635
258.216376	2053.754002	17.989376	-0.049637	2.538226
258.193207	2045.773761	17.994381	-0.049628	2.533789
258.240961	2037.807445	17.999386	-0.049632	2.529358
258.119857	2029.844138	18.004391	-0.049604	2.524908
257.962165	2021.914961	18.009395	-0.049570	2.520467
257.958044	2013.964334	18.014400	-0.049564	2.516016
257.658215	2005.970776	18.019405	-0.049503	2.511513
257.796035	1997.968103	18.024410	-0.049523	2.507028
257.830964	1990.005900	18.029415	-0.049525	2.502550
257.586336	1982.072017	18.034419	-0.049474	2.498060
257.608859	1974.121447	18.039424	-0.049473	2.493572
257.496330	1966.125681	18.044429	-0.049447	2.489040
257.323304	1958.176295	18.049434	-0.049410	2.484522
257.282455	1950.224917	18.054439	-0.049397	2.480004
257.148845	1942.286634	18.059443	-0.049367	2.475479
257.209989	1934.289778	18.064448	-0.049374	2.470926
257.079529	1926.319680	18.069453	-0.049344	2.466366
257.281691	1918.339641	18.074458	-0.049377	2.461816
257.135451	1910.402221	18.079463	-0.049344	2.457257
257.143401	1902.423359	18.084467	-0.049341	2.452676
257.061304	1894.468180	18.089472	-0.049320	2.448094
256.978234	1886.506147	18.094477	-0.049300	2.443500
256.984501	1878.566867	18.099482	-0.049296	2.438916
256.864250	1870.621640	18.104487	-0.049268	2.434311
256.681128	1862.577622	18.109491	-0.049229	2.429635
256.628774	1854.635103	18.114496	-0.049214	2.425019
256.458976	1846.691326	18.119501	-0.049178	2.420385
256.411937	1838.749857	18.124506	-0.049164	2.415752
256.470396	1830.764025	18.129511	-0.049170	2.411092
256.440010	1822.802424	18.134515	-0.049159	2.406431
256.411555	1814.858130	18.139520	-0.049148	2.401771
256.411823	1806.903413	18.144525	-0.049143	2.397099
256.332707	1798.942174	18.149530	-0.049124	2.392407
256.326874	1790.964351	18.154535	-0.049117	2.387701
256.087295	1783.025002	18.159539	-0.049068	2.382991
256.115342	1775.075207	18.164544	-0.049068	2.378286
255.941098	1767.114569	18.169549	-0.049030	2.373550
256.049708	1759.126762	18.174554	-0.049045	2.368810
255.937840	1751.196502	18.179559	-0.049019	2.364077
255.934264	1743.239931	18.184563	-0.049014	2.359328
255.860083	1735.298448	18.189568	-0.048995	2.354573
255.680878	1727.310439	18.194573	-0.048956	2.349772
255.677945	1719.364667	18.199578	-0.048951	2.345000
255.656879	1711.412630	18.204583	-0.048942	2.340214
255.667177	1703.466670	18.209587	-0.048938	2.335424
255.504381	1695.513493	18.214592	-0.048903	2.330605
255.379332	1687.547009	18.219597	-0.048875	2.325772
255.354572	1679.617190	18.224602	-0.048865	2.320959
255.492401	1671.657060	18.229607	-0.048886	2.316131
255.244523	1663.701269	18.234611	-0.048834	2.311263
255.134754	1655.747618	18.239616	-0.048809	2.306398
255.206226	1647.778888	18.244621	-0.048817	2.301529
255.284274	1639.825043	18.249626	-0.048826	2.296659
255.024561	1631.889915	18.254631	-0.048773	2.291761
255.034790	1623.926227	18.259635	-0.048770	2.286859
255.137578	1615.992136	18.264640	-0.048784	2.281972
254.972478	1608.061172	18.269645	-0.048748	2.277053
254.830516	1600.069021	18.274650	-0.048716	2.272088
254.696632	1592.089291	18.279655	-0.048686	2.267121
254.539986	1584.153075	18.284659	-0.048652	2.262167
254.654921	1576.214215	18.289664	-0.048669	2.257225
254.581696	1568.254153	18.294669	-0.048650	2.252242
254.584418	1560.301940	18.299674	-0.048645	2.247260
254.426114	1552.375592	18.304679	-0.048611	2.242268
254.306803	1544.453629	18.309683	-0.048583	2.237272
254.412003	1536.481781	18.314688	-0.048598	2.232253
254.306481	1528.519963	18.319693	-0.048573	2.227210
254.282573	1520.579095	18.324698	-0.048564	2.222176
254.306586	1512.636742	18.329703	-0.048563	2.217134
254.161739	1504.682952	18.334707	-0.048531	2.212059
254.153678	1496.757621	18.339712	-0.048524	2.207002
253.874667	1488.826862	18.344717	-0.048467	2.201905
254.127338	1480.869689	18.349722	-0.048509	2.196828
254.031378	1472.908288	18.354727	-0.048486	2.191704
253.710818	1464.976934	18.359731	-0.048421	2.186568
253.973387	1457.006364	18.364736	-0.048465	2.181447
253.707042	1449.102212	18.369741	-0.048411	2.176309
253.478519	1441.177640	18.374746	-0.048363	2.171149
253.723500	1433.187312	18.379751	-0.048404	2.165977
253.608962	1425.263880	18.384755	-0.048377	2.160804
253.495760	1417.363120	18.389760	-0.048351	2.155632
253.457539	1409.379730	18.394765	-0.048339	2.150402
253.581602	1401.408045	18.399770	-0.048357	2.145181
253.487026	1393.499946	18.404775	-0.048334	2.139969
253.331544	1385.575444	18.409779	-0.048300	2.134728
253.393589	1377.620453	18.414784	-0.048306	2.129474
253.246040	1369.705236	18.419789	-0.048274	2.124213
253.151073	1361.796527	18.424794	-0.048251	2.118949
252.952803	1353.866453	18.429799	-0.048209	2.113648
253.020778	1345.841459	18.434803	-0.048217	2.108295
252.932281	1337.925720	18.439808	-0.048195	2.102987
252.602516	1330.027018	18.444813	-0.048129	2.097653
252.742561	1322.054933	18.449818	-0.048150	2.092302
252.766274	1314.101022	18.454823	-0.048149	2.086939
252.384259	1306.228002	18.459827	-0.048073	2.081576
252.361240	1298.317405	18.464832	-0.048063	2.076209
252.469192	1290.330243	18.469837	-0.048078	2.070789
252.493309	1282.380673	18.474842	-0.048078	2.065373
252.330959	1274.479799	18.479847	-0.048043	2.059956
252.322751	1266.559321	18.484851	-0.048036	2.054528
252.470041	1258.597994	18.489856	-0.048058	2.049073
252.243116	1250.688547	18.494861	-0.048011	2.043601
252.102551	1242.791384	18.499866	-0.047980	2.038131
252.105863	1234.850266	18.504871	-0.047975	2.032631
251.936978	1226.907675	18.509875	-0.047939	2.027098
251.908884	1218.987641	18.514880	-0.047928	2.021579
251.748240	1211.070822	18.519885	-0.047893	2.016034
251.699423	1203.135560	18.524890	-0.047879	2.010472
251.722385	1195.194346	18.529895	-0.047878	2.004898
251.884133	1187.256625	18.534899	-0.047904	1.999325
251.678428	1179.377227	18.539904	-0.047860	1.993740
251.519884	1171.429401	18.544909	-0.047826	1.988095
251.541376	1163.503839	18.549914	-0.047825	1.982469
251.474926	1155.606371	18.554919	-0.047807	1.976838
251.423906	1147.664531	18.559923	-0.047792	1.971160
251.450506	1139.746412	18.564928	-0.047792	1.965492
251.391059	1131.839415	18.569933	-0.047776	1.959805
251.302571	1123.936146	18.574938	-0.047755	1.954102
251.161574	1115.982526	18.579943	-0.047723	1.948340
251.066875	1108.057410	18.584947	-0.047701	1.942586
250.964704	1100.171096	18.589952	-0.047677	1.936843
250.784700	1092.246804	18.594957	-0.047638	1.931047
250.600542	1084.349181	18.599962	-0.047599	1.925252
250.712225	1076.411327	18.604967	-0.047614	1.919442
250.492200	1068.514164	18.609971	-0.047568	1.913608
250.501274	1060.596062	18.614976	-0.047565	1.907766
250.570720	1052.652189	18.619981	-0.047573	1.901894
250.331902	1044.787423	18.624986	-0.047523	1.896028
250.354852	1036.857033	18.629991	-0.047522	1.890125
250.210235	1028.956992	18.634995	-0.047490	1.884206
250.360671	1021.047607	18.640000	-0.047513	1.878296
250.061175	1013.161174	18.645005	-0.047453	1.872332
250.023496	1005.224848	18.650010	-0.047441	1.866342
250.109617	997.314875	18.655015	-0.047451	1.860367
249.948035	989.434178	18.660019	-0.047416	1.854366
249.847487	981.518393	18.665024	-0.047393	1.848326
249.875266	973.600510	18.670029	-0.047393	1.842279
249.831141	965.724467	18.675034	-0.047379	1.836236
249.591310	957.834704	18.680039	-0.047330	1.830140
249.320582	949.955153	18.685043	-0.047274	1.824027
249.486598	942.032960	18.690048	-0.047300	1.817913
249.399546	934.131110	18.695053	-0.047279	1.811763
249.338850	926.236464	18.700058	-0.047262	1.805602
249.387406	918.355478	18.705063	-0.047266	1.799443
249.348366	910.433741	18.710067	-0.047254	1.793220
249.079346	902.530213	18.715072	-0.047199	1.786962
249.096081	894.623850	18.720077	-0.047197	1.780715
249.018521	886.764532	18.725082	-0.047178	1.774471
248.809059	878.888225	18.730087	-0.047134	1.768176
248.746953	870.999815	18.735091	-0.047117	1.761867
248.870427	863.106465	18.740096	-0.047135	1.755554
248.683057	855.220727	18.745101	-0.047095	1.749185
248.519133	847.350524	18.750106	-0.047059	1.742809
248.502919	839.471700	18.755111	-0.047051	1.736421
248.545084	831.560210	18.760115	-0.047054	1.729990
248.501904	823.706314	18.765120	-0.047041	1.723571
248.422264	815.834923	18.770125	-0.047021	1.717109
248.339715	807.948760	18.775130	-0.047001	1.710611
248.060935	800.101789	18.780135	-0.046944	1.704094
247.937088	792.233382	18.785139	-0.046916	1.697555
248.185997	784.310700	18.790144	-0.046957	1.690994
247.992350	776.451839	18.795149	-0.046916	1.684402
247.950348	768.598213	18.800154	-0.046903	1.677809
247.948885	760.718881	18.805159	-0.046898	1.671174
247.912322	752.830650	18.810163	-0.046886	1.664500
247.804794	745.007689	18.815168	-0.046861	1.657845
247.800553	737.113857	18.820173	-0.046855	1.651117
247.708379	729.268321	18.825178	-0.046833	1.644391
247.685442	721.423942	18.830183	-0.046823	1.637647
247.364116	713.554362	18.835187	-0.046759	1.630813
247.310151	705.682706	18.840192	-0.046744	1.623985
247.263682	697.825221	18.845197	-0.046730	1.617141
247.278039	689.954694	18.850202	-0.046727	1.610266
247.186018	682.117709	18.855207	-0.046705	1.603376
247.054744	674.290341	18.860211	-0.046676	1.596458
247.102592	666.416978	18.865216	-0.046680	1.589496
246.914404	658.585479	18.870221	-0.046640	1.582506
246.949123	650.743039	18.875226	-0.046641	1.575507
246.944407	642.887518	18.880231	-0.046635	1.568460
246.717933	635.073648	18.885235	-0.046588	1.561386
246.741778	627.246811	18.890240	-0.046587	1.554305
246.656398	619.383807	18.895245	-0.046567	1.547142
246.553674	611.565664	18.900250	-0.046542	1.539985
246.569849	603.729488	18.905255	-0.046540	1.532795
246.557676	595.878850	18.910259	-0.046533	1.525554
246.268898	588.118622	18.915264	-0.046474	1.518320
246.032673	580.299083	18.920269	-0.046425	1.511004
246.239058	572.430149	18.925274	-0.046459	1.503674
246.059809	564.641799	18.930279	-0.046420	1.496325
245.980098	556.813102	18.935283	-0.046401	1.488916
246.007032	549.001990	18.940288	-0.046401	1.481504
245.804780	541.213845	18.945293	-0.046358	1.474040
245.673625	533.367757	18.950298	-0.046328	1.466494
245.450115	525.597937	18.955303	-0.046282	1.458968
245.449154	517.769796	18.960307	-0.046277	1.451382
245.377858	509.976945	18.965312	-0.046258	1.443779
245.223342	502.203219	18.970317	-0.046225	1.436141
245.190853	494.393412	18.975322	-0.046214	1.428446
245.331100	486.573352	18.980327	-0.046235	1.420728
245.063394	478.825841	18.985331	-0.046180	1.412973
245.074947	471.030246	18.990336	-0.046177	1.405173
244.913001	463.276065	18.995341	-0.046142	1.397342
245.004794	455.459380	19.000346	-0.046154	1.389446
244.899187	447.694263	19.005351	-0.046129	1.381525
244.821295	439.929709	19.010355	-0.046110	1.373563
244.805978	432.153783	19.015360	-0.046102	1.365553
244.656216	424.421717	19.020365	-0.046069	1.357519
244.501661	416.666386	19.025370	-0.046036	1.349411
244.470930	408.900760	19.030375	-0.046025	1.341266
244.143386	401.198618	19.035379	-0.045959	1.333085
244.266989	393.417975	19.040384	-0.045977	1.324850
244.152792	385.696654	19.045389	-0.045951	1.316585
244.037461	377.842869	19.050394	-0.045924	1.308124
243.911304	370.117885	19.055399	-0.045896	1.299746
243.879020	362.384425	19.060403	-0.045885	1.291322
243.784690	354.683139	19.065408	-0.045862	1.282866
243.513774	347.006701	19.070413	-0.045807	1.274349
243.596156	339.259388	19.075418	-0.045817	1.265761
243.593506	331.562142	19.080423	-0.045812	1.257155
243.290973	323.892040	19.085427	-0.045751	1.248464
243.238197	316.204823	19.090432	-0.045736	1.239739
243.207367	308.497514	19.095437	-0.045725	1.230934
243.116193	300.807616	19.100442	-0.045703	1.222074
242.818295	293.175625	19.105447	-0.045643	1.213176
242.814732	285.477294	19.110451	-0.045637	1.204192
242.841462	277.814239	19.115456	-0.045638	1.195189
242.846105	270.121508	19.120461	-0.045634	1.186078
242.945574	262.462226	19.125466	-0.045647	1.176955
242.747862	254.836787	19.130471	-0.045605	1.167741
242.594999	247.219404	19.135475	-0.045572	1.158473
242.702662	239.539627	19.140480	-0.045587	1.149108
242.596639	231.908021	19.145485	-0.045563	1.139680
242.249742	224.345758	19.150490	-0.045493	1.130209
242.107158	216.748287	19.155495	-0.045462	1.120657
242.031923	209.145274	19.160499	-0.045443	1.111031
241.970008	201.554206	19.165504	-0.045426	1.101339
241.625875	194.010657	19.170509	-0.045358	1.091559
241.575231	186.432800	19.175514	-0.045343	1.081712
241.426686	178.884268	19.180519	-0.045311	1.071791
241.148689	171.337287	19.185523	-0.045254	1.061749
241.112211	163.791391	19.190528	-0.045243	1.051669
241.106751	156.230864	19.195533	-0.045237	1.041479
240.852467	148.750346	19.200538	-0.045185	1.031238
240.825426	141.225593	19.205543	-0.045175	1.020888
240.566522	133.755233	19.210547	-0.045122	1.010452
240.476204	126.277221	19.215552	-0.045100	0.999937
240.229470	118.802979	19.220557	-0.045049	0.989277
239.896668	111.367866	19.225562	-0.044983	0.978535
239.578343	103.950792	19.230567	-0.044919	0.967704
238.847279	96.618974	19.235571	-0.044778	0.956770
238.334983	89.246355	19.240576	-0.044678	0.945705
237.721384	81.916966	19.245581	-0.044559	0.934547
237.132970	74.585215	19.250586	-0.044445	0.923257
236.624246	67.262716	19.255591	-0.044345	0.911863
235.943929	60.192458	19.260595	-0.044214	0.900672