Tue Mar 23 11:14:06 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.296991	-0.041470	0.000000	-0.000037	0.722373

0.305202	-0.043483	0.005005	-0.000039	0.722372
0.135367	-0.015826	0.010010	-0.000007	0.722367
0.158235	-0.016712	0.015014	-0.000011	0.722373
0.199952	-0.027670	0.020019	-0.000019	0.722367
0.204123	-0.025148	0.025024	-0.000020	0.722373
0.395945	-0.057980	0.030029	-0.000056	0.722376
0.390799	-0.061191	0.035034	-0.000055	0.722368
0.597322	-0.092587	0.040038	-0.000093	0.722379
0.221771	-0.031050	0.045043	-0.000024	0.722368
0.324962	-0.045719	0.050048	-0.000043	0.722376
0.321757	-0.044825	0.055053	-0.000042	0.722377
0.387893	-0.062077	0.060058	-0.000055	0.722366
0.492083	-0.135572	0.065062	-0.000074	0.722258
0.292436	-0.193659	0.070067	-0.000037	0.722074
0.188886	-0.174464	0.075072	-0.000018	0.722076
0.045547	-0.146796	0.080077	0.000009	0.722080
0.205453	-0.177800	0.085082	-0.000021	0.722075
0.418612	-0.212128	0.090086	-0.000061	0.722083
0.155480	-0.170044	0.095091	-0.000012	0.722074
0.271874	-0.289176	0.100096	-0.000034	0.721880
0.228583	-0.347376	0.105101	-0.000026	0.721751
0.018489	-0.313779	0.110106	0.000013	0.721744
0.108959	-0.323845	0.115110	-0.000004	0.721756
0.186970	-0.343128	0.120115	-0.000018	0.721745
0.134747	-0.390755	0.125120	-0.000008	0.721633
0.032335	-0.468371	0.130125	0.000011	0.721445
0.105415	-0.484948	0.135130	-0.000003	0.721438
0.192589	-0.494788	0.140134	-0.000019	0.721449
0.067296	-0.477040	0.145139	0.000004	0.721441
0.281192	-0.664900	0.150144	-0.000036	0.721146
0.034894	-0.629732	0.155149	0.000010	0.721129
-0.023877	-0.620810	0.160154	0.000021	0.721126
0.130277	-0.655113	0.165158	-0.000008	0.721113
0.273206	-0.799143	0.170163	-0.000035	0.720880
0.219161	-0.788445	0.175168	-0.000025	0.720882
0.170252	-0.777947	0.180173	-0.000016	0.720886
0.088282	-0.893395	0.185178	-0.000000	0.720630
0.227767	-0.959290	0.190182	-0.000026	0.720549
0.047248	-0.929364	0.195187	0.000007	0.720545
0.225311	-1.055227	0.200192	-0.000026	0.720360
0.103094	-1.096739	0.205197	-0.000003	0.720235
-0.041761	-1.076648	0.210202	0.000024	0.720224
-0.019591	-1.181961	0.215206	0.000019	0.720024
0.033828	-1.254082	0.220211	0.000009	0.719901
0.023392	-1.251229	0.225216	0.000011	0.719903
-0.142910	-1.350967	0.230221	0.000042	0.719649
-0.124324	-1.377311	0.235226	0.000039	0.719603
0.009410	-1.429815	0.240230	0.000014	0.719547
-0.196784	-1.532792	0.245235	0.000052	0.719271
-0.401329	-1.495574	0.250240	0.000090	0.719273
-0.330929	-1.596920	0.255245	0.000077	0.719098
-0.436203	-1.647585	0.260250	0.000097	0.718961
-0.392449	-1.661264	0.265254	0.000088	0.718950
-0.398904	-1.814553	0.270259	0.000090	0.718645
-0.253463	-1.840881	0.275264	0.000062	0.718644
-0.303590	-1.930450	0.280269	0.000072	0.718450
-0.421496	-1.957425	0.285274	0.000094	0.718355
-0.263908	-2.051191	0.290278	0.000064	0.718226
-0.295763	-2.150947	0.295283	0.000070	0.718018
-0.380553	-2.171626	0.300288	0.000086	0.717947
-0.338217	-2.298529	0.305293	0.000078	0.717711
-0.610078	-2.272693	0.310298	0.000129	0.717667
-1.694662	-2.220449	0.315302	0.000330	0.717388
-2.342959	-2.109925	0.320307	0.000451	0.717379
-2.636501	-2.133479	0.325312	0.000506	0.717229
-3.559797	-2.038434	0.330317	0.000677	0.717092
-3.401258	-2.071791	0.335322	0.000648	0.717082
-3.354370	-2.147222	0.340326	0.000639	0.716949
-4.751028	-1.998636	0.345331	0.000899	0.716751
-4.283390	-2.079312	0.350336	0.000812	0.716756
-4.306290	-2.071838	0.355341	0.000816	0.716763
-5.253158	-2.057395	0.360346	0.000992	0.716458
-4.967167	-2.109585	0.365350	0.000939	0.716456
-5.227472	-2.067871	0.370355	0.000987	0.716447
-5.406888	-2.050729	0.375360	0.001021	0.716417
-5.758677	-2.129032	0.380365	0.001086	0.716138
-5.958520	-2.098083	0.385370	0.001123	0.716129
-6.322122	-2.030209	0.390374	0.001191	0.716136
-6.195984	-2.055151	0.395379	0.001167	0.716131
-6.559125	-2.097156	0.400384	0.001235	0.715920
-6.807539	-2.067713	0.405389	0.001281	0.715890
-7.031734	-2.032069	0.410394	0.001323	0.715882
-6.956669	-2.042324	0.415398	0.001309	0.715888
-6.916255	-2.095345	0.420403	0.001301	0.715798
-8.000682	-2.027996	0.425408	0.001503	0.715548
-7.789378	-2.064721	0.430413	0.001463	0.715550
-8.301498	-1.976259	0.435418	0.001559	0.715545
-7.791205	-2.063442	0.440422	0.001464	0.715553
-7.985124	-2.036573	0.445427	0.001500	0.715537
-8.834256	-2.037830	0.450432	0.001658	0.715235
-8.567721	-2.083449	0.455437	0.001608	0.715239
-9.160216	-1.982280	0.460442	0.001718	0.715230
-8.819258	-2.040094	0.465446	0.001655	0.715236
-8.860415	-2.036141	0.470451	0.001662	0.715230
-9.373419	-1.982328	0.475456	0.001758	0.715155
-9.756243	-2.035334	0.480461	0.001829	0.714915
-9.531583	-2.079867	0.485466	0.001787	0.714906
-9.886271	-2.011811	0.490470	0.001853	0.714916
-10.036017	-1.988319	0.495475	0.001881	0.714910
-9.884058	-2.014083	0.500480	0.001852	0.714913
-9.453609	-2.108638	0.505485	0.001772	0.714877
-10.679068	-2.026283	0.510490	0.002000	0.714608
-10.550688	-2.043408	0.515494	0.001976	0.714619
-10.811482	-1.999387	0.520499	0.002025	0.714614
-10.792232	-2.004187	0.525504	0.002021	0.714612
-10.776979	-2.003716	0.530509	0.002018	0.714618
-10.946512	-1.978308	0.535514	0.002050	0.714609
-10.675123	-2.127002	0.540518	0.001999	0.714410
-12.126034	-1.933651	0.545523	0.002269	0.714281
-11.730705	-2.003475	0.550528	0.002195	0.714282
-11.381866	-2.065646	0.555533	0.002130	0.714282
-12.020061	-1.955695	0.560538	0.002249	0.714275
-11.725780	-2.003828	0.565542	0.002194	0.714283
-11.159423	-2.108005	0.570547	0.002089	0.714277
-12.002029	-2.099686	0.575552	0.002246	0.713995
-12.492184	-2.021559	0.580557	0.002337	0.713977
-12.538740	-2.018248	0.585562	0.002345	0.713967
-12.120561	-2.087825	0.590566	0.002267	0.713977
-12.610998	-2.003993	0.595571	0.002359	0.713971
-12.584883	-2.009151	0.600576	0.002354	0.713970
-12.160093	-2.142840	0.605581	0.002275	0.713854
-13.800082	-1.952676	0.610586	0.002580	0.713652
-13.257752	-2.044922	0.615590	0.002479	0.713661
-13.330750	-2.037291	0.620595	0.002492	0.713650
-13.467794	-2.011697	0.625600	0.002518	0.713653
-13.526619	-1.998388	0.630605	0.002528	0.713658
-13.516636	-2.005343	0.635610	0.002527	0.713648
-13.173862	-2.126083	0.640614	0.002463	0.713530
-14.243930	-2.021265	0.645619	0.002662	0.713359
-14.418427	-1.990098	0.650624	0.002694	0.713359
-14.252265	-2.017889	0.655629	0.002663	0.713363
-14.356053	-2.001632	0.660634	0.002682	0.713359
-14.416450	-1.986671	0.665638	0.002694	0.713367
-14.589622	-1.958917	0.670643	0.002726	0.713361
-14.343627	-2.044548	0.675648	0.002680	0.713278
-15.260149	-2.004493	0.680653	0.002851	0.713033
-15.052676	-2.046035	0.685658	0.002812	0.713024
-15.087483	-2.035635	0.690662	0.002818	0.713033
-15.259831	-2.007634	0.695667	0.002850	0.713028
-15.359929	-1.990464	0.700672	0.002869	0.713026
-15.004885	-2.051434	0.705677	0.002803	0.713031
-15.393604	-2.020056	0.710682	0.002875	0.712956
-16.398814	-1.960965	0.715686	0.003062	0.712717
-16.095554	-2.018237	0.720691	0.003005	0.712711
-16.405148	-1.962375	0.725696	0.003063	0.712712
-16.275237	-1.981869	0.730701	0.003039	0.712720
-16.532008	-1.942236	0.735706	0.003086	0.712708
-16.007632	-2.030747	0.740710	0.002989	0.712718
-16.084642	-2.021453	0.745715	0.003003	0.712709
-16.516465	-2.050397	0.750720	0.003083	0.712498
-17.158136	-1.987087	0.755725	0.003203	0.712397
-17.035263	-2.014926	0.760730	0.003180	0.712385
-17.105145	-1.997498	0.765734	0.003193	0.712395
-17.174668	-1.987419	0.770739	0.003206	0.712391
-17.196025	-1.986470	0.775744	0.003209	0.712385
-17.020647	-2.015397	0.780749	0.003177	0.712390
-17.355182	-2.008948	0.785754	0.003239	0.712284
-18.129587	-1.962344	0.790758	0.003383	0.712102
-18.016536	-1.986239	0.795763	0.003362	0.712095
-18.491052	-1.900368	0.800768	0.003450	0.712098
-17.952388	-1.994683	0.805773	0.003350	0.712101
-17.924648	-2.003693	0.810778	0.003345	0.712093
-18.278241	-1.935840	0.815782	0.003410	0.712103
-18.135386	-1.965358	0.820787	0.003384	0.712095
-18.260532	-2.072754	0.825792	0.003407	0.711837
-19.129929	-1.949368	0.830797	0.003569	0.711774
-19.535886	-1.881697	0.835802	0.003644	0.711765
-18.819938	-2.006034	0.840806	0.003511	0.711771
-18.875135	-1.998309	0.845811	0.003521	0.711767
-19.089495	-1.960233	0.850816	0.003561	0.711767
-18.782807	-2.011540	0.855821	0.003504	0.711774
-19.117551	-2.023238	0.860826	0.003566	0.711632
-19.998748	-1.950121	0.865830	0.003730	0.711465
-19.559936	-2.030251	0.870835	0.003648	0.711461
-19.908491	-1.969556	0.875840	0.003713	0.711458
-19.849506	-1.976736	0.880845	0.003702	0.711465
-19.852153	-1.980915	0.885850	0.003702	0.711456
-19.775496	-1.991282	0.890854	0.003688	0.711463
-19.817610	-2.058522	0.895859	0.003696	0.711314
-20.944493	-1.945774	0.900864	0.003905	0.711138
-20.688537	-1.987228	0.905869	0.003858	0.711147
-20.757064	-1.979042	0.910874	0.003870	0.711139
-21.054035	-1.922687	0.915878	0.003926	0.711146
-21.013169	-1.932779	0.920883	0.003918	0.711140
-20.905875	-1.949975	0.925888	0.003898	0.711144
-20.835017	-1.960640	0.930893	0.003885	0.711148
-21.427385	-1.980780	0.935898	0.003995	0.710898
-21.730538	-1.935988	0.940902	0.004051	0.710879
-21.347880	-2.006428	0.945907	0.003980	0.710875
-21.446112	-1.989234	0.950912	0.003998	0.710874
-21.835086	-1.918521	0.955917	0.004070	0.710877
-21.792965	-1.929812	0.960922	0.004063	0.710870
-21.583401	-1.962495	0.965926	0.004023	0.710879
-21.999438	-2.035996	0.970931	0.004101	0.710585
-22.478172	-1.979916	0.975936	0.004190	0.710527
-22.274636	-2.009965	0.980941	0.004152	0.710539
-22.571994	-1.961942	0.985946	0.004207	0.710529
-22.513441	-1.969284	0.990950	0.004196	0.710536
-22.330386	-2.003965	0.995955	0.004162	0.710532
-22.651806	-1.946068	1.000960	0.004222	0.710533
-23.040106	-2.030525	1.005965	0.004294	0.710226
-23.118770	-2.020996	1.010970	0.004309	0.710217
-23.314191	-1.983166	1.015974	0.004345	0.710224
-23.468313	-1.958590	1.020979	0.004374	0.710218
-23.617670	-1.932131	1.025984	0.004401	0.710218
-23.174914	-2.007891	1.030989	0.004319	0.710224
-23.381517	-1.985405	1.035994	0.004357	0.710196
-24.075160	-2.008627	1.040998	0.004486	0.709902
-24.249694	-1.979281	1.046003	0.004519	0.709899
-24.477019	-1.941270	1.051008	0.004561	0.709894
-24.257170	-1.978097	1.056013	0.004520	0.709899
-24.338854	-1.966583	1.061018	0.004535	0.709893
-24.049908	-2.014550	1.066022	0.004481	0.709900
-24.164853	-1.995666	1.071027	0.004503	0.709897
-24.724679	-2.045824	1.076032	0.004607	0.709597
-24.660749	-2.053193	1.081037	0.004595	0.709606
-25.475310	-1.912769	1.086042	0.004746	0.709596
-25.181330	-1.960856	1.091046	0.004691	0.709605
-24.940637	-2.006431	1.096051	0.004647	0.709600
-25.340873	-1.934721	1.101056	0.004721	0.709601
-25.276284	-1.949659	1.106061	0.004709	0.709594
-25.745006	-2.032436	1.111066	0.004796	0.709261
-26.145969	-1.953577	1.116070	0.004871	0.709276
-26.521822	-1.890032	1.121075	0.004941	0.709270
-26.099788	-1.964293	1.126080	0.004862	0.709272
-25.801099	-2.017161	1.131085	0.004806	0.709273
-26.202507	-1.948556	1.136090	0.004881	0.709267
-26.308467	-1.925694	1.141094	0.004901	0.709275
-26.093697	-2.045209	1.146099	0.004861	0.709112
-27.174290	-1.929714	1.151104	0.005062	0.708958
-26.900683	-1.974139	1.156109	0.005011	0.708967
-27.046390	-1.952848	1.161114	0.005038	0.708958
-26.994347	-1.960052	1.166118	0.005028	0.708962
-26.899464	-1.978359	1.171123	0.005010	0.708960
-27.226735	-1.921675	1.176128	0.005071	0.708956
-27.028812	-2.014654	1.181133	0.005034	0.708841
-28.112887	-1.922306	1.186138	0.005236	0.708639
-27.628122	-2.002803	1.191142	0.005146	0.708651
-27.644285	-2.004165	1.196147	0.005148	0.708643
-28.073347	-1.929496	1.201152	0.005228	0.708639
-27.871081	-1.960549	1.206157	0.005191	0.708649
-27.823835	-1.974652	1.211162	0.005182	0.708638
-27.552015	-2.083617	1.216166	0.005131	0.708517
-29.033696	-1.901674	1.221171	0.005407	0.708353
-29.060721	-1.899308	1.226176	0.005412	0.708348
-28.527077	-1.989921	1.231181	0.005312	0.708357
-28.848571	-1.937845	1.236186	0.005372	0.708347
-29.009276	-1.904764	1.241190	0.005402	0.708356
-28.563852	-1.984874	1.246195	0.005319	0.708355
-28.789407	-1.966793	1.251200	0.005361	0.708310
-29.590535	-1.967712	1.256205	0.005510	0.708022
-29.814066	-1.933089	1.261210	0.005551	0.708012
-29.607577	-1.966652	1.266214	0.005513	0.708019
-29.476288	-1.990472	1.271219	0.005488	0.708018
-29.815143	-1.932730	1.276224	0.005551	0.708013
-29.500984	-1.984468	1.281229	0.005493	0.708022
-29.594583	-1.978954	1.286234	0.005510	0.707999
-30.365875	-1.987260	1.291238	0.005654	0.707707
-30.360858	-1.991574	1.296243	0.005653	0.707700
-30.931459	-1.891130	1.301248	0.005759	0.707698
-30.773960	-1.915537	1.306253	0.005729	0.707706
-30.633284	-1.944648	1.311258	0.005703	0.707698
-30.366891	-1.988889	1.316262	0.005654	0.707704
-30.497814	-1.966215	1.321267	0.005678	0.707703
-31.290457	-1.951284	1.326272	0.005825	0.707450
-31.474451	-1.951076	1.331277	0.005860	0.707384
-31.360787	-1.977005	1.336282	0.005838	0.707373
-31.742545	-1.906052	1.341286	0.005909	0.707379
-31.803240	-1.893598	1.346291	0.005920	0.707383
-31.383383	-1.970051	1.351296	0.005842	0.707380
-31.394436	-1.965978	1.356301	0.005844	0.707384
-31.946162	-1.906064	1.361306	0.005947	0.707307
-32.428612	-1.929934	1.366310	0.006037	0.707087
-31.899407	-2.024825	1.371315	0.005938	0.707086
-32.729436	-1.877714	1.376320	0.006092	0.707084
-32.242926	-1.962004	1.381325	0.006002	0.707089
-32.258777	-1.964345	1.386330	0.006005	0.707079
-32.548765	-1.909163	1.391334	0.006059	0.707086
-32.319105	-1.987514	1.396339	0.006016	0.707011
-33.152120	-1.966650	1.401344	0.006171	0.706755
-33.171623	-1.959674	1.406349	0.006174	0.706762
-33.585057	-1.892515	1.411354	0.006251	0.706749
-33.115805	-1.972140	1.416358	0.006164	0.706757
-33.178532	-1.963094	1.421363	0.006175	0.706753
-33.893656	-1.837079	1.426368	0.006308	0.706750
-33.144874	-1.966366	1.431373	0.006169	0.706759
-33.621699	-2.039531	1.436378	0.006258	0.706441
-34.303167	-1.913958	1.441382	0.006385	0.706450
-34.154872	-1.940617	1.446387	0.006357	0.706449
-33.784950	-2.008212	1.451392	0.006288	0.706446
-34.042567	-1.957868	1.456397	0.006336	0.706455
-34.172939	-1.939172	1.461402	0.006360	0.706446
-33.969390	-2.011361	1.466406	0.006322	0.706374
-34.681337	-2.004458	1.471411	0.006455	0.706133
-34.770772	-1.988320	1.476416	0.006471	0.706134
-34.952969	-1.951536	1.481421	0.006505	0.706142
-35.089490	-1.932984	1.486426	0.006530	0.706131
-35.077937	-1.931896	1.491430	0.006528	0.706137
-35.004534	-1.947109	1.496435	0.006514	0.706133
-35.059314	-1.988220	1.501440	0.006524	0.706031
-35.867822	-1.924123	1.506445	0.006675	0.705870
-35.681005	-1.961490	1.511450	0.006640	0.705862
-35.735558	-1.949513	1.516454	0.006650	0.705867
-35.670108	-1.960670	1.521459	0.006638	0.705868
-35.840396	-1.933614	1.526464	0.006669	0.705862
-35.729245	-1.947873	1.531469	0.006649	0.705873
-35.830951	-2.037307	1.536474	0.006668	0.705657
-36.689675	-1.944941	1.541478	0.006827	0.705535
-36.755386	-1.934932	1.546483	0.006840	0.705531
-36.765075	-1.935955	1.551488	0.006841	0.705526
-36.635179	-1.956699	1.556493	0.006817	0.705531
-36.724550	-1.943985	1.561498	0.006834	0.705525
-36.812612	-1.925300	1.566502	0.006850	0.705531
-36.889928	-2.015343	1.571507	0.006864	0.705322
-37.965608	-1.878886	1.576512	0.007064	0.705211
-37.525584	-1.953591	1.581517	0.006982	0.705219
-37.688305	-1.927995	1.586522	0.007013	0.705212
-37.693718	-1.923306	1.591526	0.007014	0.705219
-37.270619	-2.000653	1.596531	0.006935	0.705216
-37.278845	-2.000501	1.601536	0.006936	0.705213
-37.464824	-2.082636	1.606541	0.006971	0.704981
-38.854242	-1.879611	1.611546	0.007229	0.704891
-38.375690	-1.961845	1.616550	0.007140	0.704898
-38.103205	-2.011960	1.621555	0.007089	0.704895
-38.521845	-1.939584	1.626560	0.007167	0.704890
-38.525580	-1.936048	1.631565	0.007168	0.704896
-38.212387	-1.996246	1.636570	0.007109	0.704888
-38.850480	-2.012995	1.641574	0.007228	0.704625
-39.289231	-1.949075	1.646579	0.007310	0.704596
-39.547086	-1.904504	1.651584	0.007358	0.704594
-39.104648	-1.979297	1.656589	0.007275	0.704602
-39.507772	-1.912821	1.661594	0.007350	0.704591
-39.338005	-1.940097	1.666598	0.007319	0.704597
-39.172623	-1.971353	1.671603	0.007288	0.704594
-39.911647	-1.981857	1.676608	0.007425	0.704307
-40.257463	-1.938480	1.681613	0.007490	0.704271
-40.326226	-1.931058	1.686618	0.007502	0.704261
-40.129929	-1.963335	1.691622	0.007466	0.704267
-40.041453	-1.979490	1.696627	0.007449	0.704266
-40.131244	-1.965300	1.701632	0.007466	0.704263
-39.914505	-2.000873	1.706637	0.007425	0.704269
-40.900201	-1.971552	1.711642	0.007609	0.703974
-41.209943	-1.925969	1.716646	0.007666	0.703955
-40.859522	-1.986147	1.721651	0.007601	0.703959
-40.703530	-2.017896	1.726656	0.007572	0.703951
-41.091217	-1.944608	1.731661	0.007644	0.703960
-41.309561	-1.908701	1.736666	0.007685	0.703954
-41.021348	-1.958758	1.741670	0.007631	0.703957
-41.434906	-2.022806	1.746675	0.007708	0.703679
-42.302710	-1.889687	1.751680	0.007869	0.703636
-41.827239	-1.972120	1.756685	0.007781	0.703641
-41.636911	-2.008326	1.761690	0.007745	0.703636
-41.932382	-1.954222	1.766694	0.007800	0.703639
-42.006072	-1.940735	1.771699	0.007814	0.703640
-41.815078	-1.978374	1.776704	0.007778	0.703633
-42.567086	-1.978659	1.781709	0.007918	0.703362
-42.884454	-1.935223	1.786714	0.007977	0.703335
-42.876458	-1.931891	1.791718	0.007975	0.703345
-42.804688	-1.944759	1.796723	0.007962	0.703345
-42.940849	-1.921759	1.801728	0.007987	0.703343
-42.641423	-1.971614	1.806733	0.007931	0.703350
-42.979435	-1.915995	1.811738	0.007994	0.703341
-43.360323	-1.976503	1.816742	0.008065	0.703082
-43.789080	-1.936653	1.821747	0.008145	0.703008
-43.691509	-1.956554	1.826752	0.008127	0.703003
-43.551384	-1.975079	1.831757	0.008101	0.703016
-43.855482	-1.925965	1.836762	0.008157	0.703006
-43.617716	-1.965952	1.841766	0.008113	0.703011
-43.540037	-1.981960	1.846771	0.008098	0.703007
-44.292454	-1.969607	1.851776	0.008238	0.702761
-44.542379	-1.956290	1.856781	0.008285	0.702698
-44.418261	-1.981618	1.861786	0.008261	0.702692
-44.560511	-1.954248	1.866790	0.008288	0.702696
-44.204479	-2.016054	1.871795	0.008222	0.702699
-44.155816	-2.027776	1.876800	0.008212	0.702693
-44.270628	-2.036728	1.881805	0.008234	0.702634
-45.385298	-1.967367	1.886810	0.008441	0.702373
-44.905658	-2.050632	1.891814	0.008352	0.702377
-45.524334	-1.942304	1.896819	0.008467	0.702373
-45.738605	-1.907112	1.901824	0.008507	0.702367
-45.150365	-2.006882	1.906829	0.008397	0.702378
-45.571793	-1.935956	1.911834	0.008475	0.702370
-45.605408	-1.955586	1.916838	0.008482	0.702318
-45.800641	-2.039850	1.921843	0.008518	0.702077
-46.104027	-1.988229	1.926848	0.008574	0.702072
-46.471534	-1.916883	1.931853	0.008643	0.702084
-46.498040	-1.915935	1.936858	0.008648	0.702077
-46.163953	-1.973717	1.941862	0.008585	0.702081
-46.215560	-1.966018	1.946867	0.008595	0.702078
-46.616575	-1.931093	1.951872	0.008669	0.702004
-46.774224	-2.030021	1.956877	0.008699	0.701747
-46.764704	-2.035532	1.961882	0.008697	0.701739
-47.517886	-1.897164	1.966886	0.008837	0.701748
-47.175094	-1.957696	1.971891	0.008773	0.701749
-46.845976	-2.020532	1.976896	0.008712	0.701741
-46.831682	-2.019337	1.981901	0.008709	0.701749
-47.285230	-2.014890	1.986906	0.008793	0.701594
-48.234810	-1.921565	1.991910	0.008970	0.701440
-47.901321	-1.981442	1.996915	0.008908	0.701440
-48.049287	-1.955286	2.001920	0.008935	0.701439

-48.122440	-1.943357	2.011917	0.008949	0.701437
-47.902880	-1.983344	2.021914	0.008908	0.701436
-48.256990	-1.922790	2.031910	0.008974	0.701431
-48.568473	-2.017562	2.041907	0.009031	0.701127
-48.712619	-1.897997	2.051904	0.009058	0.701317
-48.351310	-1.945121	2.061901	0.008991	0.701353
-48.390569	-1.896402	2.071898	0.008998	0.701437
-48.048263	-1.957231	2.081894	0.008934	0.701438
-48.043280	-1.957959	2.091891	0.008933	0.701439
-48.278856	-1.915528	2.101888	0.008977	0.701440
-48.063511	-1.956191	2.111885	0.008936	0.701436
-48.217371	-1.928098	2.121882	0.008965	0.701437
-48.159852	-1.938076	2.131878	0.008954	0.701438
-48.034397	-1.914858	2.141875	0.008930	0.701531
-47.093897	-1.976333	2.151872	0.008755	0.701746
-47.156583	-1.966425	2.161869	0.008767	0.701744
-47.413893	-1.918460	2.171866	0.008814	0.701748
-47.293968	-1.939718	2.181862	0.008792	0.701749
-46.734582	-1.937344	2.191859	0.008688	0.701956
-46.213278	-1.970253	2.201856	0.008590	0.702078
-46.369714	-1.944405	2.211853	0.008619	0.702074
-46.365037	-1.945657	2.221850	0.008618	0.702073
-46.199860	-1.927429	2.231846	0.008587	0.702170
-45.429276	-1.963682	2.241843	0.008444	0.702375
-45.567640	-1.941018	2.251840	0.008469	0.702371
-45.557298	-1.943976	2.261837	0.008467	0.702369
-44.915744	-1.956499	2.271834	0.008348	0.702575
-44.428629	-1.984220	2.281830	0.008257	0.702695
-44.592821	-1.955175	2.291827	0.008287	0.702695
-44.532822	-1.967372	2.301824	0.008276	0.702692
-43.991476	-1.941829	2.311821	0.008175	0.702939
-43.939272	-1.918020	2.321818	0.008165	0.703006
-43.686656	-1.963046	2.331814	0.008118	0.703007
-43.662134	-1.916503	2.341811	0.008113	0.703110
-42.859357	-1.942787	2.351808	0.007964	0.703346
-42.786890	-1.958987	2.361805	0.007950	0.703340
-42.941835	-1.931901	2.371802	0.007979	0.703339
-42.192552	-1.971099	2.381798	0.007839	0.703530
-42.063154	-1.940849	2.391795	0.007815	0.703638
-42.076991	-1.938221	2.401792	0.007817	0.703638
-41.965229	-1.935564	2.411789	0.007796	0.703684
-41.318048	-1.919093	2.421786	0.007676	0.703951
-41.072024	-1.962825	2.431782	0.007630	0.703951
-41.088988	-1.960452	2.441779	0.007633	0.703950
-40.577755	-1.948097	2.451776	0.007537	0.704159
-40.293043	-1.948543	2.461773	0.007484	0.704261
-40.440553	-1.922668	2.471770	0.007511	0.704260
-40.181767	-1.926895	2.481766	0.007463	0.704345
-39.611607	-1.905440	2.491763	0.007357	0.704594
-39.315393	-1.958968	2.501760	0.007301	0.704592
-39.410525	-1.941539	2.511757	0.007319	0.704594
-38.829324	-1.924099	2.521754	0.007211	0.704838
-38.513808	-1.952752	2.531750	0.007152	0.704894
-38.487666	-1.958102	2.541747	0.007147	0.704893
-38.451589	-1.920962	2.551744	0.007140	0.704981
-37.710723	-1.935672	2.561741	0.007002	0.705217
-37.530630	-1.969783	2.571738	0.006968	0.705214
-37.577534	-1.960988	2.581734	0.006977	0.705215
-37.091942	-1.936911	2.591731	0.006886	0.705438
-36.795194	-1.946118	2.601728	0.006831	0.705526
-36.864948	-1.933950	2.611725	0.006843	0.705526
-36.764468	-1.908403	2.621722	0.006825	0.705614
-35.709692	-1.971603	2.631718	0.006628	0.705865
-35.939665	-1.930103	2.641715	0.006671	0.705866
-35.686998	-1.978197	2.651712	0.006624	0.705860
-35.503317	-1.913256	2.661709	0.006589	0.706057
-35.122396	-1.946439	2.671706	0.006518	0.706127
-35.193600	-1.933236	2.681702	0.006531	0.706129
-34.940804	-1.914235	2.691699	0.006484	0.706258
-34.021861	-1.985797	2.701696	0.006313	0.706443
-34.397230	-1.919862	2.711693	0.006382	0.706442
-34.318845	-1.930520	2.721690	0.006368	0.706449
-33.574569	-1.912352	2.731686	0.006229	0.706752
-33.363680	-1.948295	2.741683	0.006190	0.706756
-33.254675	-1.968414	2.751680	0.006169	0.706755
-32.986655	-1.921329	2.761677	0.006119	0.706946
-32.147976	-2.003704	2.771674	0.005963	0.707081
-32.472080	-1.943056	2.781670	0.006023	0.707087
-32.458278	-1.945236	2.791667	0.006020	0.707088
-31.703490	-1.940004	2.801664	0.005879	0.707368
-31.671828	-1.941084	2.811661	0.005873	0.707378
-31.745119	-1.929027	2.821658	0.005887	0.707376
-31.237202	-1.922307	2.831654	0.005792	0.707572
-30.710025	-1.950737	2.841651	0.005694	0.707703
-30.803304	-1.935508	2.851648	0.005711	0.707701
-30.753378	-1.919623	2.861645	0.005702	0.707751
-29.881865	-1.944285	2.871642	0.005539	0.708013
-29.945934	-1.932704	2.881638	0.005551	0.708014
-29.911242	-1.937436	2.891635	0.005544	0.708017
-29.233880	-1.931773	2.901632	0.005418	0.708271
-28.949776	-1.943913	2.911629	0.005365	0.708348
-28.721153	-1.984840	2.921626	0.005322	0.708348
-29.054863	-1.909458	2.931622	0.005384	0.708380
-28.331910	-1.907479	2.941619	0.005249	0.708643
-28.169014	-1.936343	2.951616	0.005219	0.708643
-28.250350	-1.923791	2.961613	0.005234	0.708640
-27.666185	-1.898668	2.971610	0.005125	0.708899
-27.468256	-1.904350	2.981606	0.005088	0.708958
-27.003886	-1.985879	2.991603	0.005001	0.708961
-27.205003	-1.894732	3.001600	0.005039	0.709072
-26.140404	-1.988005	3.011597	0.004840	0.709266
-26.407096	-1.940358	3.021594	0.004890	0.709266
-26.359570	-1.948897	3.031590	0.004881	0.709266
-25.847646	-1.918705	3.041587	0.004785	0.709510
-25.490823	-1.939586	3.051584	0.004719	0.709595
-25.491917	-1.940867	3.061581	0.004719	0.709593
-25.277326	-1.940267	3.071578	0.004679	0.709671
-24.906446	-1.894286	3.081574	0.004609	0.709895
-24.436333	-1.977300	3.091571	0.004522	0.709897
-24.687353	-1.934949	3.101568	0.004568	0.709892
-23.861996	-1.950088	3.111565	0.004415	0.710156
-23.838679	-1.923975	3.121562	0.004410	0.710217
-23.822738	-1.926494	3.131558	0.004407	0.710218
-23.586641	-1.919013	3.141555	0.004363	0.710318
-22.920884	-1.928865	3.151552	0.004239	0.710535
-22.600967	-1.987812	3.161549	0.004179	0.710532
-22.926327	-1.928934	3.171546	0.004239	0.710534
-22.129068	-1.954274	3.181542	0.004091	0.710767
-21.860756	-1.947521	3.191539	0.004041	0.710876
-21.953234	-1.931309	3.201536	0.004058	0.710876
-21.771279	-1.958749	3.211533	0.004024	0.710886
-21.409616	-1.897021	3.221530	0.003956	0.711139
-21.098847	-1.951480	3.231526	0.003898	0.711141
-20.887926	-1.989872	3.241523	0.003859	0.711139
-20.821899	-1.899470	3.251520	0.003846	0.711344
-20.195754	-1.955519	3.261517	0.003730	0.711455
-20.550733	-1.892032	3.271514	0.003796	0.711455
-20.144700	-1.924722	3.281510	0.003720	0.711535
-19.526169	-1.919097	3.291507	0.003604	0.711766
-19.579045	-1.911392	3.301504	0.003614	0.711763
-19.497229	-1.919454	3.311501	0.003599	0.711776
-18.674446	-1.907953	3.321498	0.003445	0.712092
-18.553668	-1.929970	3.331494	0.003423	0.712091
-18.361291	-1.962743	3.341491	0.003387	0.712094
-18.400431	-1.880755	3.351488	0.003394	0.712244
-17.482180	-1.971427	3.361485	0.003223	0.712390
-18.012553	-1.877678	3.371482	0.003321	0.712389
-17.574319	-1.939266	3.381478	0.003240	0.712422
-17.096513	-1.877531	3.391475	0.003150	0.712715
-16.744858	-1.940481	3.401472	0.003085	0.712714
-16.705333	-1.948729	3.411469	0.003077	0.712712
-16.338850	-1.914047	3.421466	0.003009	0.712911
-15.956334	-1.925456	3.431462	0.002938	0.713025
-16.055614	-1.906073	3.441459	0.002956	0.713028
-15.979709	-1.884644	3.451456	0.002942	0.713098
-15.007825	-1.926131	3.461453	0.002761	0.713361
-15.179653	-1.895905	3.471450	0.002792	0.713360
-15.071873	-1.913956	3.481446	0.002772	0.713363
-14.546009	-1.898137	3.491443	0.002674	0.713581
-14.084738	-1.941199	3.501440	0.002588	0.713659
-14.044062	-1.950479	3.511437	0.002580	0.713655
-13.998483	-1.951279	3.521434	0.002572	0.713670
-13.190084	-1.942533	3.531430	0.002421	0.713974
-13.068821	-1.964281	3.541427	0.002398	0.713974
-13.165802	-1.946525	3.551424	0.002416	0.713975
-13.171122	-1.885728	3.561421	0.002417	0.714094
-12.412605	-1.927590	3.571418	0.002276	0.714280
-12.097613	-1.983373	3.581414	0.002217	0.714281
-12.188429	-1.965024	3.591411	0.002234	0.714286
-11.391051	-1.986513	3.601408	0.002085	0.714525
-11.362642	-1.945684	3.611405	0.002079	0.714617
-11.243223	-1.967850	3.621402	0.002057	0.714615
-11.068618	-1.999256	3.631398	0.002024	0.714615
-10.746136	-1.930506	3.641395	0.001964	0.714866
-10.161073	-2.008960	3.651392	0.001855	0.714917
-10.340618	-1.978624	3.661389	0.001888	0.714914
-10.303486	-1.968615	3.671386	0.001881	0.714948
-9.395995	-1.985528	3.681382	0.001712	0.715235
-9.319106	-1.997756	3.691379	0.001698	0.715238
-9.187156	-2.021957	3.701376	0.001673	0.715237
-9.320968	-1.944268	3.711373	0.001698	0.715344
-8.206902	-2.040169	3.721370	0.001490	0.715548
-8.253622	-2.030932	3.731366	0.001499	0.715550
-8.131999	-2.052742	3.741363	0.001476	0.715550
-7.938068	-2.053067	3.751360	0.001440	0.715618
-7.296308	-2.032239	3.761357	0.001320	0.715886
-7.052419	-2.076691	3.771354	0.001275	0.715885
-7.051977	-2.076839	3.781350	0.001274	0.715885
-7.271091	-2.022941	3.791347	0.001315	0.715915
-6.452807	-2.057194	3.801344	0.001162	0.716136
-6.634421	-2.025430	3.811341	0.001196	0.716135
-6.325179	-2.079668	3.821338	0.001138	0.716137
-6.280876	-2.002390	3.831334	0.001130	0.716306
-5.389204	-2.086618	3.841331	0.000964	0.716454
-5.556719	-2.055986	3.851328	0.000995	0.716456
-5.599714	-2.051356	3.861325	0.001003	0.716450
-4.688642	-2.067661	3.871322	0.000833	0.716740
-4.809491	-2.037128	3.881318	0.000855	0.716758
-4.555676	-2.080229	3.891315	0.000808	0.716762
-4.461359	-2.040878	3.901312	0.000790	0.716874
-3.692714	-2.069599	3.911309	0.000647	0.717088
-3.622371	-2.084249	3.921306	0.000634	0.717084
-3.494543	-2.105029	3.931302	0.000610	0.717088
-3.471159	-2.039311	3.941299	0.000605	0.717227
-2.740975	-2.089455	3.951296	0.000469	0.717385
-3.206835	-2.008023	3.961293	0.000555	0.717382
-2.625471	-2.111544	3.971290	0.000447	0.717383
-2.565234	-1.959913	3.981286	0.000436	0.717704
-2.406917	-1.987819	3.991283	0.000406	0.717705
-2.103665	-2.042129	4.001280	0.000349	0.717705
-2.091879	-1.901053	4.011277	0.000347	0.717988
-1.574465	-1.979341	4.021274	0.000251	0.718016
-1.515449	-1.989445	4.031270	0.000239	0.718017
-1.897460	-1.758755	4.041267	0.000310	0.718338
-1.116610	-1.886714	4.051264	0.000165	0.718361
-1.927010	-1.675680	4.061261	0.000315	0.718493
-1.277020	-1.713683	4.071258	0.000194	0.718646
-1.163661	-1.691661	4.081254	0.000173	0.718730
-1.537367	-1.505773	4.091251	0.000242	0.718966
-0.806393	-1.583924	4.101248	0.000106	0.719069
-1.084562	-1.431116	4.111245	0.000158	0.719273
-0.851500	-1.395145	4.121242	0.000114	0.719426
-0.819668	-1.309336	4.131238	0.000108	0.719607
-0.895444	-1.185194	4.141235	0.000122	0.719825
-0.673075	-1.163833	4.151232	0.000080	0.719946
-0.894848	-0.980125	4.161229	0.000121	0.720230
-1.060960	-0.842264	4.171226	0.000152	0.720444
-0.525372	-0.836847	4.181222	0.000052	0.720642
-0.435976	-0.728453	4.191219	0.000035	0.720887
-0.002819	-0.695121	4.201216	-0.000046	0.721105
-0.274049	-0.554583	4.211213	0.000005	0.721287
-0.285802	-0.436891	4.221210	0.000007	0.721514
-0.228580	-0.325997	4.231206	-0.000004	0.721753
-0.350494	-0.137396	4.241203	0.000018	0.722081
-0.161538	-0.039314	4.251200	-0.000017	0.722340
-0.088678	0.090668	4.261197	-0.000031	0.722621
0.000000	0.236154	4.271194	-0.000048	0.722938

0.071288	0.869203	4.276198	-0.000062	0.724204
0.078503	2.129521	4.281203	-0.000064	0.726672
0.337976	3.935915	4.286208	-0.000113	0.730280
0.813193	6.263234	4.291213	-0.000204	0.734951
1.088417	9.131984	4.296218	-0.000257	0.740563
1.629608	12.439985	4.301222	-0.000360	0.747056
2.180414	16.201768	4.306227	-0.000465	0.754351
2.646722	20.383336	4.311232	-0.000554	0.762329
3.272502	24.950343	4.316237	-0.000674	0.770986
3.671230	29.913415	4.321242	-0.000752	0.780194
4.881438	35.092583	4.326246	-0.000980	0.789941
5.943299	40.627248	4.331251	-0.001182	0.800152
6.589689	46.541150	4.336256	-0.001306	0.810770
7.276297	52.733820	4.341261	-0.001438	0.821743
7.886781	59.215074	4.346266	-0.001556	0.833040
9.242506	65.786171	4.351270	-0.001813	0.844558
9.979712	72.708069	4.356275	-0.001955	0.856320
10.625587	79.836565	4.361280	-0.002080	0.868234
11.248362	87.171044	4.366285	-0.002200	0.880311
11.905865	94.660983	4.371290	-0.002328	0.892482
12.512759	102.327909	4.376294	-0.002446	0.904752
12.989692	110.156197	4.381299	-0.002540	0.917072
13.435874	118.099628	4.386304	-0.002628	0.929395
14.286473	126.096278	4.391309	-0.002792	0.941744
15.180883	134.193140	4.396314	-0.002964	0.954093
15.826112	142.408401	4.401318	-0.003089	0.966393
16.558078	150.689753	4.406323	-0.003231	0.978656
17.232922	159.068420	4.411328	-0.003362	0.990892
18.048524	167.468134	4.416333	-0.003520	1.003043
18.613206	175.948334	4.421338	-0.003630	1.015099
19.419651	184.423994	4.426342	-0.003786	1.027065
19.993133	192.990898	4.431347	-0.003899	1.038962
20.656572	201.550808	4.436352	-0.004028	1.050736
21.326377	210.154741	4.441357	-0.004158	1.062439
21.962240	218.783377	4.446362	-0.004282	1.074039
22.333469	227.445321	4.451366	-0.004357	1.085498
23.337384	236.025112	4.456371	-0.004550	1.096873
23.522713	244.734702	4.461376	-0.004590	1.108116
24.114852	253.385529	4.466381	-0.004706	1.119260
24.575262	262.043146	4.471386	-0.004797	1.130274
25.292812	270.660611	4.476390	-0.004937	1.141186
26.017951	279.307491	4.481395	-0.005078	1.152032
26.385914	287.961411	4.486400	-0.005152	1.162711
27.304731	296.533302	4.491405	-0.005329	1.173307
27.881346	305.137747	4.496410	-0.005442	1.183777
28.482027	313.743614	4.501414	-0.005559	1.194161
29.286803	322.292959	4.506419	-0.005715	1.204430
29.635379	330.906522	4.511424	-0.005785	1.214596
30.271654	339.470168	4.516429	-0.005909	1.224676
30.968189	348.019219	4.521434	-0.006045	1.234669
31.619729	356.532741	4.526438	-0.006172	1.244531
32.039493	365.099437	4.531443	-0.006255	1.254332
32.500469	373.613194	4.536448	-0.006347	1.264005
33.265457	382.106350	4.541453	-0.006495	1.273639
34.193786	390.528077	4.546458	-0.006673	1.283151
34.935077	399.002502	4.551462	-0.006817	1.292616
35.575978	407.470996	4.556467	-0.006942	1.301987
35.977283	416.032675	4.561472	-0.007022	1.311348
36.751549	424.499402	4.566477	-0.007172	1.320608
37.352161	432.904006	4.571482	-0.007289	1.329705
38.096577	441.290519	4.576486	-0.007434	1.338747
38.595728	449.712075	4.581491	-0.007532	1.347722
38.903367	458.154176	4.586496	-0.007595	1.356625
39.467587	466.535174	4.591501	-0.007706	1.365451
39.890581	474.936744	4.596506	-0.007790	1.374217
40.884923	483.239778	4.601510	-0.007981	1.382923
41.769032	491.581287	4.606515	-0.008151	1.391596
42.040899	499.981604	4.611520	-0.008207	1.400170
42.799922	508.297291	4.616525	-0.008354	1.408689
43.222918	516.654643	4.621530	-0.008438	1.417142
43.734844	524.991077	4.626534	-0.008539	1.425539
44.461905	533.309001	4.631539	-0.008680	1.433903
44.690895	541.658854	4.636544	-0.008728	1.442169
45.221608	549.975927	4.641549	-0.008832	1.450404
45.906694	558.265921	4.646554	-0.008965	1.458591
46.180491	566.601667	4.651558	-0.009022	1.466711
46.838004	574.933535	4.656563	-0.009150	1.474842
47.116052	583.234455	4.661568	-0.009207	1.482840
47.657514	591.503591	4.666573	-0.009313	1.490806
48.021469	599.794212	4.671578	-0.009386	1.498722
48.368851	608.066690	4.676582	-0.009457	1.506577
49.084155	616.311603	4.681587	-0.009595	1.514421
49.452879	624.567395	4.686592	-0.009669	1.522182
50.159445	632.792775	4.691597	-0.009806	1.529926
50.832662	641.029937	4.696602	-0.009937	1.537636
51.103221	649.310916	4.701606	-0.009993	1.545289
51.583588	657.586732	4.706611	-0.010088	1.552930
51.966177	665.815576	4.711616	-0.010165	1.560476
52.490591	674.050827	4.716621	-0.010268	1.568012
52.866702	682.294750	4.721626	-0.010343	1.575498
53.247538	690.530368	4.726630	-0.010419	1.582942
53.905767	698.731740	4.731635	-0.010547	1.590360
54.250347	706.975078	4.736640	-0.010617	1.597736
54.847078	715.161697	4.741645	-0.010734	1.605064
55.178141	723.406468	4.746650	-0.010801	1.612372
55.831970	731.578364	4.751654	-0.010928	1.619628
56.300649	739.785023	4.756659	-0.011021	1.626856
56.661691	748.065025	4.761664	-0.011093	1.634101
57.224103	756.242890	4.766669	-0.011203	1.641253
57.331103	764.473298	4.771674	-0.011229	1.648356
57.725989	772.667520	4.776678	-0.011308	1.655438
58.320879	780.824147	4.781683	-0.011424	1.662484
58.497802	789.049983	4.786688	-0.011462	1.669502
59.062097	797.228069	4.791693	-0.011573	1.676503
59.743517	805.354935	4.796698	-0.011705	1.683447
60.092752	813.552962	4.801702	-0.011775	1.690377
60.672966	821.733639	4.806707	-0.011889	1.697296
60.974984	829.920641	4.811712	-0.011950	1.704154
61.512996	838.096674	4.816717	-0.012056	1.711007
62.007882	846.271788	4.821722	-0.012154	1.717826
62.527030	854.408658	4.826726	-0.012256	1.724590
62.889920	862.603116	4.831731	-0.012329	1.731354
63.467353	870.747782	4.836736	-0.012442	1.738078
64.100651	878.887417	4.841741	-0.012565	1.744779
64.853921	887.031598	4.846746	-0.012710	1.751473
65.002818	895.252019	4.851750	-0.012744	1.758127
65.501110	903.402657	4.856755	-0.012842	1.764744
65.868206	911.578082	4.861760	-0.012916	1.771339
66.236710	919.768480	4.866765	-0.012990	1.777921
66.437212	927.934281	4.871770	-0.013032	1.784439
67.215139	936.067912	4.876774	-0.013183	1.790979
67.725110	944.250162	4.881779	-0.013283	1.797500
67.881044	952.398484	4.886784	-0.013317	1.803928
68.613077	960.489699	4.891789	-0.013459	1.810357
69.241122	968.610625	4.896794	-0.013581	1.816775
69.388592	976.780037	4.901798	-0.013614	1.823150
69.651803	984.961624	4.906803	-0.013669	1.829525
70.361841	993.049372	4.911808	-0.013806	1.835860
70.736373	1001.197919	4.916813	-0.013881	1.842179
71.239032	1009.319336	4.921818	-0.013980	1.848471
71.523122	1017.489887	4.926822	-0.014039	1.854753
71.985487	1025.624473	4.931827	-0.014130	1.861007
72.278230	1033.772624	4.936832	-0.014190	1.867231
72.634090	1041.954541	4.941837	-0.014262	1.873467
73.132654	1050.046418	4.946842	-0.014360	1.879630
73.312466	1058.189461	4.951846	-0.014399	1.885776
73.401607	1066.377191	4.956851	-0.014421	1.891924
73.853258	1074.460965	4.961856	-0.014510	1.898016
74.178007	1082.588883	4.966861	-0.014576	1.904107
74.337560	1090.736321	4.971866	-0.014611	1.910174
74.789796	1098.840074	4.976870	-0.014701	1.916223
75.211213	1106.942928	4.981875	-0.014784	1.922248
75.275023	1115.090380	4.986880	-0.014802	1.928247
75.922027	1123.187727	4.991885	-0.014928	1.934256
76.367536	1131.282281	4.996890	-0.015016	1.940221
77.011078	1139.363866	5.001894	-0.015141	1.946180
77.642797	1147.511311	5.006899	-0.015264	1.952167
77.999719	1155.634996	5.011904	-0.015336	1.958089
78.371633	1163.749316	5.016909	-0.015410	1.963988
78.492585	1171.881077	5.021914	-0.015438	1.969855
78.978545	1179.979111	5.026918	-0.015534	1.975718
79.720997	1188.048173	5.031923	-0.015678	1.981571
79.829228	1196.180117	5.036928	-0.015703	1.987385
80.302074	1204.308900	5.041933	-0.015797	1.993217
80.775701	1212.386414	5.046938	-0.015890	1.998996
81.639658	1220.407394	5.051942	-0.016056	2.004759
81.871921	1228.567069	5.056947	-0.016105	2.010537
82.023646	1236.712743	5.061952	-0.016139	2.016281
82.275315	1244.840524	5.066957	-0.016191	2.022005
82.512462	1252.951894	5.071962	-0.016240	2.027701
82.833975	1261.094957	5.076966	-0.016306	2.033411
83.209126	1269.190135	5.081971	-0.016381	2.039078
83.339436	1277.281151	5.086976	-0.016411	2.044701
83.797454	1285.372124	5.091981	-0.016501	2.050341
84.319358	1293.453525	5.096986	-0.016604	2.055966
84.588915	1301.537968	5.101990	-0.016659	2.061552
85.004219	1309.635852	5.106995	-0.016742	2.067147
85.504880	1317.725308	5.112000	-0.016840	2.072729
85.985039	1325.822780	5.117005	-0.016935	2.078299
86.294864	1333.920235	5.122010	-0.016998	2.083838
86.675623	1342.005705	5.127014	-0.017075	2.089360
87.169621	1350.116350	5.132019	-0.017172	2.094896
87.372771	1358.215875	5.137024	-0.017215	2.100382
87.714547	1366.316263	5.142029	-0.017284	2.105867
88.175013	1374.433972	5.147034	-0.017375	2.111361
88.949031	1382.507490	5.152038	-0.017525	2.116841
89.574043	1390.555870	5.157043	-0.017646	2.122276
89.592529	1398.677540	5.162048	-0.017655	2.127688
89.890743	1406.792965	5.167053	-0.017716	2.133108
90.434463	1414.852126	5.172058	-0.017823	2.138500
90.574583	1422.963787	5.177062	-0.017854	2.143876
91.056145	1431.045966	5.182067	-0.017949	2.149250
91.225193	1439.171477	5.187072	-0.017986	2.154610
91.547947	1447.240677	5.192077	-0.018051	2.159935
92.132762	1455.272704	5.197082	-0.018166	2.165246
92.500194	1463.357702	5.202086	-0.018239	2.170558
92.737162	1471.490185	5.207091	-0.018289	2.175876
92.834687	1479.571094	5.212096	-0.018312	2.181135
93.184717	1487.661675	5.217101	-0.018383	2.186411
93.511738	1495.758159	5.222106	-0.018449	2.191675
93.922692	1503.837567	5.227110	-0.018531	2.196924
94.502572	1511.868607	5.232115	-0.018644	2.202144
94.810090	1519.934327	5.237120	-0.018707	2.207349
95.239469	1528.022950	5.242125	-0.018792	2.212567
95.406969	1536.130306	5.247130	-0.018829	2.217762
95.876883	1544.186981	5.252134	-0.018921	2.222939
96.228098	1552.272269	5.257139	-0.018992	2.228111
96.311408	1560.402458	5.262144	-0.019013	2.233277
96.693633	1568.463923	5.267149	-0.019090	2.238413
96.925264	1576.541905	5.272154	-0.019138	2.243534
97.389539	1584.579873	5.277158	-0.019230	2.248639
97.779872	1592.691969	5.282163	-0.019308	2.253773
98.151122	1600.747257	5.287168	-0.019382	2.258857
98.499927	1608.822831	5.292173	-0.019453	2.263940
98.886231	1616.894110	5.297178	-0.019530	2.269013
99.250393	1625.041485	5.302182	-0.019603	2.274120
99.403292	1633.117652	5.307187	-0.019637	2.279153
99.294192	1641.190672	5.312192	-0.019622	2.284150
99.800236	1649.229799	5.317197	-0.019721	2.289168
100.251109	1657.290712	5.322202	-0.019811	2.294183
100.345736	1665.376335	5.327206	-0.019834	2.299173
100.594439	1673.453421	5.332211	-0.019885	2.304159
101.008203	1681.487919	5.337216	-0.019968	2.309123
101.320084	1689.590929	5.342221	-0.020031	2.314109
101.538839	1697.642725	5.347226	-0.020077	2.319045
101.927235	1705.683104	5.352230	-0.020155	2.323978
102.243171	1713.757889	5.357235	-0.020219	2.328915
102.764011	1721.815531	5.362240	-0.020321	2.333848
103.503935	1729.849026	5.367245	-0.020464	2.338774
103.917845	1737.905311	5.372250	-0.020547	2.343676
104.094064	1746.025391	5.377254	-0.020585	2.348587
104.348526	1754.155937	5.382259	-0.020638	2.353501
104.673008	1762.182597	5.387264	-0.020703	2.358348
105.061203	1770.231766	5.392269	-0.020781	2.363203
105.349266	1778.298412	5.397274	-0.020840	2.368050
105.748382	1786.369250	5.402278	-0.020920	2.372899
105.926083	1794.451381	5.407283	-0.020958	2.377727
106.118722	1802.502067	5.412288	-0.020999	2.382528
106.687574	1810.547595	5.417293	-0.021111	2.387346
106.969915	1818.637946	5.422298	-0.021169	2.392158
107.274791	1826.710047	5.427302	-0.021231	2.396951
107.549510	1834.766222	5.432307	-0.021287	2.401722
107.877841	1842.810251	5.437312	-0.021354	2.406481
108.408909	1850.870692	5.442317	-0.021458	2.411257
108.727032	1858.958599	5.447322	-0.021522	2.416022
109.115255	1866.990388	5.452326	-0.021600	2.420750
109.590568	1875.065460	5.457331	-0.021694	2.425501
109.837654	1883.140368	5.462336	-0.021745	2.430225
110.030807	1891.311881	5.467341	-0.021786	2.434991
110.478018	1899.309208	5.472346	-0.021875	2.439667
110.396572	1907.378042	5.477350	-0.021865	2.444335
110.789596	1915.424971	5.482355	-0.021944	2.449017
111.072329	1923.487368	5.487360	-0.022002	2.453691
111.356662	1931.549387	5.492365	-0.022060	2.458356
111.434158	1939.615559	5.497370	-0.022080	2.462998
111.877709	1947.637096	5.502374	-0.022168	2.467634
112.348971	1955.701511	5.507379	-0.022261	2.472288
112.419565	1963.767293	5.512384	-0.022279	2.476903
112.902275	1971.794761	5.517389	-0.022374	2.481519
113.136186	1979.857618	5.522394	-0.022423	2.486128
113.429275	1987.921628	5.527398	-0.022483	2.490733
113.664999	1996.016972	5.532403	-0.022532	2.495343
113.946847	2004.059153	5.537408	-0.022590	2.499918
114.356025	2012.099323	5.542413	-0.022672	2.504493
114.419662	2020.199115	5.547418	-0.022689	2.509068
114.838970	2028.272018	5.552422	-0.022772	2.513645
115.400822	2036.315257	5.557427	-0.022882	2.518207
115.565959	2044.334225	5.562432	-0.022918	2.522719
115.727249	2052.404412	5.567437	-0.022954	2.527251
116.049968	2060.457448	5.572442	-0.023019	2.531777
116.359518	2068.530418	5.577446	-0.023082	2.536305
116.772520	2076.567297	5.582451	-0.023164	2.540812
117.026136	2084.588081	5.587456	-0.023217	2.545290
117.498070	2092.651513	5.592461	-0.023310	2.549800
117.611077	2100.755175	5.597466	-0.023336	2.554299
117.801688	2108.786586	5.602470	-0.023377	2.558755
118.214354	2116.833556	5.607475	-0.023459	2.563228
118.496775	2124.857957	5.612480	-0.023517	2.567671
118.834744	2132.932612	5.617485	-0.023586	2.572138
119.148179	2140.995875	5.622490	-0.023649	2.576589
119.309707	2149.046730	5.627494	-0.023685	2.581015
119.567979	2157.106832	5.632499	-0.023738	2.585446
119.720893	2165.159778	5.637504	-0.023772	2.589857
120.091541	2173.403877	5.642509	-0.023846	2.594380
120.523253	2181.387355	5.647514	-0.023932	2.598757
120.556381	2189.397607	5.652518	-0.023943	2.603115
121.084522	2197.405363	5.657523	-0.024047	2.607497
121.334342	2205.428818	5.662528	-0.024099	2.611862
121.522111	2213.497499	5.667533	-0.024139	2.616239
121.958399	2221.505733	5.672538	-0.024226	2.620593
122.262388	2229.524454	5.677542	-0.024288	2.624937
122.764786	2237.578083	5.682547	-0.024387	2.629305
122.968917	2245.650094	5.687552	-0.024430	2.633656
123.220754	2253.703813	5.692557	-0.024482	2.637994
123.589888	2261.732949	5.697562	-0.024556	2.642318
123.771080	2269.783262	5.702566	-0.024595	2.646635
124.115438	2277.847687	5.707571	-0.024665	2.650962
124.155529	2285.934166	5.712576	-0.024677	2.655275
124.600274	2293.944052	5.717581	-0.024766	2.659566
125.103544	2301.980618	5.722586	-0.024865	2.663867
125.254827	2310.035483	5.727590	-0.024898	2.668149
125.422747	2318.123793	5.732595	-0.024935	2.672443
125.385901	2326.208610	5.737600	-0.024933	2.676715
125.936626	2334.189809	5.742605	-0.025041	2.680963
126.154200	2342.215853	5.747610	-0.025087	2.685206
126.136831	2350.312100	5.752614	-0.025089	2.689465
126.694507	2358.350902	5.757619	-0.025198	2.693723
127.135250	2366.362573	5.762624	-0.025286	2.697953
127.517552	2374.398257	5.767629	-0.025362	2.702184
127.926812	2382.448924	5.772634	-0.025444	2.706419
128.231692	2390.490190	5.777638	-0.025506	2.710636
128.570050	2398.580939	5.782643	-0.025574	2.714874
128.495608	2406.628567	5.787648	-0.025565	2.719057
128.744553	2414.669992	5.792653	-0.025617	2.723250
129.188585	2422.685174	5.797658	-0.025705	2.727436
129.267808	2430.755512	5.802662	-0.025725	2.731621
129.729527	2438.806974	5.807667	-0.025816	2.735813
130.069941	2446.819421	5.812672	-0.025885	2.739971
130.066919	2454.899841	5.817677	-0.025890	2.744137
130.479911	2462.932100	5.822682	-0.025972	2.748297
130.823302	2471.003180	5.827686	-0.026041	2.752466
131.076785	2479.110633	5.832691	-0.026094	2.756643
131.321141	2487.104788	5.837696	-0.026145	2.760754
131.713279	2495.084588	5.842701	-0.026223	2.764861
132.167186	2503.134100	5.847706	-0.026313	2.769001
132.427931	2511.179826	5.852710	-0.026367	2.773121
132.900166	2519.221072	5.857715	-0.026460	2.777245
133.171846	2527.260343	5.862720	-0.026516	2.781350
133.366048	2535.321240	5.867725	-0.026557	2.785455
133.539765	2543.381115	5.872730	-0.026595	2.789553
133.819335	2551.411732	5.877734	-0.026652	2.793636
134.294503	2559.453353	5.882739	-0.026746	2.797730
134.304823	2567.494284	5.887744	-0.026753	2.801790
134.710633	2575.520073	5.892749	-0.026834	2.805860
134.995208	2583.569165	5.897754	-0.026893	2.809929
135.317905	2591.631943	5.902758	-0.026958	2.814001
135.483363	2599.697787	5.907763	-0.026994	2.818059
135.712635	2607.705128	5.912768	-0.027042	2.822086
135.714075	2615.783059	5.917773	-0.027048	2.826129
136.074076	2623.809317	5.922778	-0.027120	2.830161
136.377427	2631.875566	5.927782	-0.027182	2.834204
136.706333	2639.908614	5.932787	-0.027249	2.838226
136.783989	2647.940219	5.937792	-0.027268	2.842227
137.185494	2655.957333	5.942797	-0.027348	2.846234
137.489004	2663.993236	5.947802	-0.027410	2.850239
137.634138	2672.057168	5.952806	-0.027443	2.854243
137.936961	2680.098395	5.957811	-0.027504	2.858240
138.267335	2688.116352	5.962816	-0.027571	2.862220
138.582998	2696.141608	5.967821	-0.027635	2.866198
138.650790	2704.195731	5.972826	-0.027653	2.870171
138.947145	2712.269862	5.977830	-0.027714	2.874160
139.307010	2720.305084	5.982835	-0.027786	2.878129
139.491277	2728.318904	5.987840	-0.027826	2.882071
139.792540	2736.371633	5.992845	-0.027887	2.886034
140.104621	2744.402486	5.997850	-0.027950	2.889981
140.434989	2752.455900	6.002854	-0.028017	2.893935
140.434450	2760.530127	6.007859	-0.028022	2.897876
140.645960	2768.556111	6.012864	-0.028067	2.901799
141.029103	2776.572290	6.017869	-0.028144	2.905721
141.256937	2784.627480	6.022874	-0.028192	2.909648
141.985364	2792.683922	6.027878	-0.028333	2.913598
142.378630	2800.712284	6.032883	-0.028411	2.917510
142.593595	2808.727858	6.037888	-0.028456	2.921402
142.681294	2816.749364	6.042893	-0.028478	2.925284
142.946155	2824.794676	6.047898	-0.028533	2.929182
143.261091	2832.818207	6.052902	-0.028597	2.933067
143.344257	2840.918534	6.057907	-0.028617	2.936972
143.610220	2848.914427	6.062912	-0.028672	2.940831
143.944639	2856.903174	6.067917	-0.028740	2.944685
144.109852	2865.001574	6.072922	-0.028776	2.948577
144.261740	2873.033283	6.077926	-0.028810	2.952432
144.643822	2881.075686	6.082931	-0.028886	2.956299
144.950598	2889.072810	6.087936	-0.028948	2.960135
145.284583	2897.107035	6.092941	-0.029016	2.963985
145.670248	2905.150966	6.097946	-0.029093	2.967837
145.701823	2913.219655	6.102950	-0.029104	2.971678
145.898643	2921.295695	6.107955	-0.029146	2.975526
145.999555	2929.299672	6.112960	-0.029170	2.979330
146.221533	2937.332747	6.117965	-0.029217	2.983148
146.555670	2945.375596	6.122970	-0.029284	2.986973
146.744541	2953.402643	6.127974	-0.029325	2.990777
147.146404	2961.478445	6.132979	-0.029405	2.994610
147.257378	2969.496701	6.137984	-0.029431	2.998397
147.384015	2977.527495	6.142989	-0.029460	3.002185
147.714858	2985.538475	6.147994	-0.029527	3.005970
147.969660	2993.549731	6.152998	-0.029580	3.009746
148.233073	3001.622890	6.158003	-0.029634	3.013547
148.265914	3009.659078	6.163008	-0.029645	3.017314
148.445053	3017.700799	6.168013	-0.029684	3.021086
148.774114	3025.715725	6.173018	-0.029751	3.024849
148.883007	3033.744882	6.178022	-0.029776	3.028602
149.452433	3041.806123	6.183027	-0.029888	3.032388
149.675192	3049.840401	6.188032	-0.029934	3.036140
149.767086	3057.864638	6.193037	-0.029957	3.039877
150.147864	3065.890621	6.198042	-0.030033	3.043623
150.339090	3073.921909	6.203046	-0.030074	3.047358
150.748326	3081.964426	6.208051	-0.030155	3.051104
150.697387	3090.018863	6.213056	-0.030151	3.054830
151.041997	3098.029914	6.218061	-0.030221	3.058549
151.261081	3106.073834	6.223066	-0.030267	3.062273
151.365202	3114.111574	6.228070	-0.030292	3.065984
151.860080	3122.168994	6.233075	-0.030389	3.069718
152.100581	3130.239150	6.238080	-0.030439	3.073441
152.300299	3138.284587	6.243085	-0.030482	3.077147
152.476921	3146.293145	6.248090	-0.030520	3.080830
152.872952	3154.238862	6.253094	-0.030599	3.084490
152.939806	3162.336480	6.258099	-0.030617	3.088199
152.992266	3170.373581	6.263104	-0.030632	3.091877
153.448648	3178.392863	6.268109	-0.030722	3.095560
153.616046	3186.394637	6.273114	-0.030759	3.099217
153.641495	3194.446845	6.278118	-0.030769	3.102887
154.040731	3202.502318	6.283123	-0.030848	3.106570
154.474659	3210.485078	6.288128	-0.030934	3.110218
154.767686	3218.544384	6.293133	-0.030994	3.113890
155.217032	3226.571723	6.298138	-0.031083	3.117550
155.310843	3234.602432	6.303142	-0.031106	3.121191
155.597070	3242.609812	6.308147	-0.031165	3.124826
155.821012	3250.657680	6.313152	-0.031212	3.128472
156.097180	3258.694706	6.318157	-0.031268	3.132111
156.160490	3266.779392	6.323162	-0.031285	3.135759
156.305575	3274.786446	6.328166	-0.031318	3.139370
156.871459	3282.804142	6.333171	-0.031428	3.143001
156.791023	3290.853961	6.338176	-0.031419	3.146613
156.947518	3298.871887	6.343181	-0.031453	3.150217
157.221718	3306.973407	6.348186	-0.031510	3.153860
157.497324	3314.950323	6.353190	-0.031566	3.157443
157.726686	3323.003085	6.358195	-0.031614	3.161054
157.662208	3330.984372	6.363200	-0.031608	3.164616
158.082701	3339.021833	6.368205	-0.031691	3.168219
158.434122	3347.055663	6.373210	-0.031762	3.171814
158.553865	3355.117462	6.378214	-0.031790	3.175408
158.831520	3363.129812	6.383219	-0.031847	3.178982
158.950281	3371.184060	6.388224	-0.031874	3.182564
159.249559	3379.178866	6.393229	-0.031935	3.186123
159.415241	3387.225768	6.398234	-0.031971	3.189695
159.724710	3395.261806	6.403238	-0.032034	3.193265
160.204094	3403.300117	6.408243	-0.032129	3.196839
160.319293	3411.327566	6.413248	-0.032155	3.200388
160.724404	3419.321113	6.418253	-0.032236	3.203931
161.036379	3427.348775	6.423258	-0.032300	3.207481
160.823156	3435.424804	6.428262	-0.032265	3.211027
161.194362	3443.457105	6.433267	-0.032340	3.214573
161.396941	3451.482206	6.438272	-0.032383	3.218106
161.681790	3459.512839	6.443277	-0.032441	3.221640
161.949686	3467.525501	6.448282	-0.032496	3.225162
162.102264	3475.554906	6.453286	-0.032530	3.228683
162.506925	3483.646979	6.458291	-0.032611	3.232237
162.663983	3491.713825	6.463296	-0.032645	3.235767
162.784788	3499.689082	6.468301	-0.032673	3.239251
163.321041	3507.688532	6.473306	-0.032778	3.242759
163.282944	3515.718785	6.478310	-0.032776	3.246253
163.683474	3523.726117	6.483315	-0.032856	3.249751
163.847035	3531.787674	6.488320	-0.032892	3.253259
164.016838	3539.824335	6.493325	-0.032929	3.256753
164.065157	3547.862037	6.498330	-0.032943	3.260238
164.437966	3555.844271	6.503334	-0.033018	3.263709
164.736939	3563.907606	6.508339	-0.033079	3.267208
164.798456	3571.946986	6.513344	-0.033096	3.270684
165.129291	3579.990196	6.518349	-0.033163	3.274168
165.179990	3588.028964	6.523354	-0.033177	3.277636
165.346683	3596.041195	6.528358	-0.033214	3.281093
165.891952	3604.020768	6.533363	-0.033320	3.284547
165.997429	3612.052710	6.538368	-0.033345	3.288002
166.060105	3620.120266	6.543373	-0.033362	3.291468
166.395625	3628.134917	6.548378	-0.033430	3.294918
166.609824	3636.144855	6.553382	-0.033475	3.298357
167.011404	3644.188990	6.558387	-0.033555	3.301815
166.879408	3652.202006	6.563392	-0.033536	3.305236
166.981097	3660.249453	6.568397	-0.033560	3.308676
167.310666	3668.306498	6.573402	-0.033627	3.312125
167.683844	3676.344089	6.578406	-0.033702	3.315565
167.747875	3684.368891	6.583411	-0.033719	3.318983
168.178249	3692.330294	6.588416	-0.033805	3.322385
168.152887	3700.359701	6.593421	-0.033805	3.325795
168.356489	3708.392124	6.598426	-0.033848	3.329212
168.554980	3716.428928	6.603430	-0.033891	3.332626
168.934461	3724.507065	6.608435	-0.033967	3.336061
168.996546	3732.500090	6.613440	-0.033984	3.339445
169.197900	3740.523236	6.618445	-0.034026	3.342843
169.466661	3748.565863	6.623450	-0.034082	3.346249
169.601945	3756.569781	6.628454	-0.034112	3.349630
169.768150	3764.654080	6.633459	-0.034148	3.353042
169.976865	3772.681475	6.638464	-0.034193	3.356429
170.361435	3780.667910	6.643469	-0.034270	3.359801
170.333199	3788.721492	6.648474	-0.034270	3.363183
170.516829	3796.741364	6.653478	-0.034309	3.366555
171.034579	3804.731376	6.658483	-0.034411	3.369923
171.018103	3812.804629	6.663488	-0.034413	3.373303
171.425534	3820.842764	6.668493	-0.034494	3.376681
171.773031	3828.848603	6.673498	-0.034564	3.380039
172.082684	3836.835831	6.678502	-0.034627	3.383385
172.304543	3844.917848	6.683507	-0.034674	3.386764
172.462213	3852.906972	6.688512	-0.034708	3.390098
172.802313	3861.023897	6.693517	-0.034777	3.393489
173.017051	3869.055886	6.698522	-0.034822	3.396837
172.932856	3877.030487	6.703526	-0.034812	3.400147
173.194185	3885.055724	6.708531	-0.034866	3.403487
173.455321	3893.049819	6.713536	-0.034920	3.406811
173.457004	3901.069452	6.718541	-0.034926	3.410133
173.945944	3909.109709	6.723546	-0.035022	3.413477
173.944050	3917.129573	6.728550	-0.035027	3.416792
174.308235	3925.146958	6.733555	-0.035100	3.420116
174.447593	3933.177037	6.738560	-0.035131	3.423434
174.943416	3941.204155	6.743565	-0.035229	3.426760
175.054925	3949.249276	6.748570	-0.035255	3.430077
175.065956	3957.285329	6.753574	-0.035262	3.433383
175.440961	3965.340010	6.758579	-0.035337	3.436706
175.602738	3973.342268	6.763584	-0.035373	3.439997
175.837722	3981.338010	6.768589	-0.035422	3.443285
176.087134	3989.392181	6.773594	-0.035474	3.446594
176.132020	3997.385138	6.778598	-0.035487	3.449868
176.357890	4005.481232	6.783603	-0.035535	3.453187
176.494825	4013.511287	6.788608	-0.035566	3.456473
176.793471	4021.481126	6.793613	-0.035626	3.459737
177.017679	4029.524267	6.798618	-0.035673	3.463024
177.348184	4037.538402	6.803622	-0.035740	3.466301
177.475191	4045.579392	6.808627	-0.035769	3.469578
177.815707	4053.637374	6.813632	-0.035838	3.472866
177.958808	4061.664834	6.818637	-0.035870	3.476132
178.093842	4069.672848	6.823642	-0.035900	3.479387
178.281811	4077.658114	6.828646	-0.035941	3.482632
178.556723	4085.657257	6.833651	-0.035997	3.485881
178.992919	4093.695459	6.838656	-0.036084	3.489149
179.350899	4101.722749	6.843661	-0.036156	3.492406
179.657147	4109.781032	6.848666	-0.036218	3.495672
179.788678	4117.786952	6.853670	-0.036248	3.498907
179.970879	4125.803426	6.858675	-0.036287	3.502146
180.034853	4133.844229	6.863680	-0.036304	3.505387
180.182637	4141.865927	6.868685	-0.036337	3.508621
180.541613	4149.919380	6.873690	-0.036409	3.511871
180.854266	4157.914024	6.878694	-0.036473	3.515092
181.224093	4165.921153	6.883699	-0.036547	3.518318
181.196320	4173.984592	6.888704	-0.036547	3.521550
181.543947	4181.946022	6.893709	-0.036617	3.524751
181.543571	4190.030009	6.898714	-0.036622	3.527987
181.592008	4198.026383	6.903718	-0.036637	3.531186
182.043800	4206.099887	6.908723	-0.036726	3.534425
182.267725	4214.141700	6.913728	-0.036773	3.537642
182.543192	4222.154212	6.918733	-0.036830	3.540846
182.794177	4230.174366	6.923738	-0.036882	3.544049
183.336214	4238.152868	6.928742	-0.036988	3.547242
183.612685	4246.211844	6.933747	-0.037045	3.550455
183.726135	4254.320141	6.938752	-0.037071	3.553680
184.189720	4262.336171	6.943757	-0.037163	3.556876
184.375625	4270.297308	6.948762	-0.037203	3.560040
184.521074	4278.308772	6.953766	-0.037235	3.563219
184.757539	4286.338182	6.958771	-0.037285	3.566405
184.908079	4294.362188	6.963776	-0.037318	3.569583
185.042358	4302.376425	6.968781	-0.037348	3.572755
185.120709	4310.426417	6.973786	-0.037368	3.575936
185.491087	4318.407134	6.978790	-0.037442	3.579095
185.806047	4326.453741	6.983795	-0.037506	3.582275
185.733093	4334.461727	6.988800	-0.037498	3.585427
186.125607	4342.487878	6.993805	-0.037576	3.588596
186.504703	4350.526240	6.998810	-0.037652	3.591767
186.505447	4358.544736	7.003814	-0.037658	3.594916
186.960338	4366.552369	7.008819	-0.037748	3.598072
187.158098	4374.573492	7.013824	-0.037790	3.601222
187.480385	4382.551488	7.018829	-0.037855	3.604356
187.647254	4390.625725	7.023834	-0.037892	3.607521
187.846209	4398.645778	7.028838	-0.037934	3.610663
187.826064	4406.741809	7.033843	-0.037935	3.613825
188.076274	4414.770054	7.038848	-0.037987	3.616966
188.384434	4422.712474	7.043853	-0.038050	3.620072
188.673467	4430.737730	7.048858	-0.038109	3.623207
188.659369	4438.779018	7.053862	-0.038112	3.626338
189.043904	4446.805369	7.058867	-0.038189	3.629470
189.389175	4454.844752	7.063872	-0.038258	3.632604
189.295554	4462.918940	7.068877	-0.038246	3.635737
189.532181	4470.935604	7.073882	-0.038296	3.638854
189.705206	4478.924115	7.078886	-0.038333	3.641955
189.937643	4486.906609	7.083891	-0.038382	3.645053
190.064618	4494.949162	7.088896	-0.038411	3.648169
190.054678	4502.992566	7.093901	-0.038414	3.651279
190.465068	4511.027424	7.098906	-0.038496	3.654393
190.608082	4519.053321	7.103910	-0.038528	3.657495
190.819411	4527.070995	7.108915	-0.038572	3.660593
191.041039	4535.072990	7.113920	-0.038619	3.663682
191.129141	4543.114269	7.118925	-0.038641	3.666780
191.423229	4551.121104	7.123930	-0.038701	3.669868
191.412829	4559.164746	7.128934	-0.038704	3.672959
191.737106	4567.195500	7.133939	-0.038770	3.676052
192.016761	4575.183199	7.138944	-0.038827	3.679124
192.043600	4583.223635	7.143949	-0.038838	3.682207
192.546493	4591.233142	7.148954	-0.038936	3.685288
192.417844	4599.251634	7.153958	-0.038918	3.688354
192.753217	4607.304539	7.158963	-0.038986	3.691442
193.212305	4615.303187	7.163968	-0.039076	3.694509
193.504294	4623.333412	7.168973	-0.039136	3.697582
193.519906	4631.374356	7.173978	-0.039144	3.700650
193.907647	4639.345619	7.178982	-0.039222	3.703698
194.239686	4647.385428	7.183987	-0.039289	3.706768
194.441085	4655.396079	7.188992	-0.039332	3.709821
194.642748	4663.488167	7.193997	-0.039375	3.712902
194.963090	4671.554052	7.199002	-0.039440	3.715974
195.140557	4679.486041	7.204006	-0.039478	3.718989
195.292812	4687.536499	7.209011	-0.039511	3.722045
195.661504	4695.486071	7.214016	-0.039585	3.725067
195.876259	4703.505540	7.219021	-0.039631	3.728108
195.999481	4711.576186	7.224026	-0.039659	3.731164
196.177960	4719.585618	7.229030	-0.039698	3.734196
196.519581	4727.646090	7.234035	-0.039766	3.737248
196.556034	4735.627101	7.239040	-0.039779	3.740261
197.045030	4743.621422	7.244045	-0.039875	3.743287
197.395138	4751.678234	7.249050	-0.039945	3.746330
197.329432	4759.692596	7.254054	-0.039938	3.749346
197.628608	4767.761657	7.259059	-0.039999	3.752388
197.984139	4775.777464	7.264064	-0.040071	3.755409
198.212526	4783.786822	7.269069	-0.040119	3.758422
198.301994	4791.819449	7.274074	-0.040141	3.761438
198.293287	4799.813682	7.279078	-0.040144	3.764435
198.732626	4807.844860	7.284083	-0.040232	3.767454
198.794794	4815.870253	7.289088	-0.040248	3.770460
199.021238	4823.925668	7.294093	-0.040296	3.773478
199.368176	4831.960406	7.299098	-0.040366	3.776488
199.535663	4839.947968	7.304102	-0.040402	3.779475
199.792426	4847.990217	7.309107	-0.040455	3.782481
200.007430	4855.994536	7.314112	-0.040501	3.785470
200.243814	4864.020794	7.319117	-0.040550	3.788465
200.471288	4872.066623	7.324122	-0.040598	3.791465
200.443108	4880.130500	7.329126	-0.040598	3.794464
200.727683	4888.127086	7.334131	-0.040656	3.797442
201.006046	4896.083344	7.339136	-0.040713	3.800403
201.268393	4904.064536	7.344141	-0.040767	3.803370
201.369282	4912.157412	7.349146	-0.040791	3.806373
201.495744	4920.122064	7.354150	-0.040820	3.809326
201.820356	4928.187928	7.359155	-0.040886	3.812319
201.792437	4936.214519	7.364160	-0.040886	3.815287
202.175513	4944.216400	7.369165	-0.040963	3.818253
202.521655	4952.227613	7.374170	-0.041033	3.821219
202.617709	4960.216156	7.379174	-0.041056	3.824169
202.836083	4968.253165	7.384179	-0.041102	3.827137
203.113758	4976.297432	7.389184	-0.041159	3.830106
203.019850	4984.334036	7.394189	-0.041147	3.833063
203.460020	4992.370869	7.399194	-0.041234	3.836029
203.682481	5000.318286	7.404198	-0.041281	3.838955
203.766591	5008.407058	7.409203	-0.041302	3.841927
203.990432	5016.345529	7.414208	-0.041348	3.844846
204.142289	5024.412457	7.419213	-0.041382	3.847807
204.512523	5032.467774	7.424218	-0.041456	3.850766
204.573554	5040.473794	7.429222	-0.041473	3.853699
204.733438	5048.556553	7.434227	-0.041508	3.856660
204.834925	5056.538559	7.439232	-0.041532	3.859580
204.959863	5064.541642	7.444237	-0.041561	3.862506
205.184108	5072.585736	7.449242	-0.041608	3.865447
205.209272	5080.610746	7.454246	-0.041618	3.868375
205.500186	5088.671396	7.459251	-0.041677	3.871319
205.580277	5096.867842	7.464256	-0.041698	3.874306
205.771148	5104.828800	7.469261	-0.041739	3.877207
206.024846	5112.732383	7.474266	-0.041791	3.880086
206.165510	5120.745004	7.479270	-0.041822	3.883000
206.583936	5128.729404	7.484275	-0.041906	3.885907
206.670036	5136.762248	7.489280	-0.041927	3.888824
206.982274	5144.755833	7.494285	-0.041990	3.891728
207.338570	5152.818771	7.499290	-0.042062	3.894656
207.614530	5160.817882	7.504294	-0.042119	3.897557
207.803655	5168.794726	7.509299	-0.042159	3.900446
207.854802	5176.847699	7.514304	-0.042174	3.903358
208.023726	5184.840192	7.519309	-0.042211	3.906248
208.344151	5192.878591	7.524314	-0.042276	3.909155
208.440812	5200.925766	7.529318	-0.042299	3.912059
208.670542	5208.944541	7.534323	-0.042347	3.914953
208.828279	5216.978169	7.539328	-0.042382	3.917849
208.861239	5224.927712	7.544333	-0.042393	3.920710
209.299418	5232.964544	7.549338	-0.042480	3.923608
209.302051	5240.978681	7.554342	-0.042486	3.926488
209.547851	5248.994538	7.559347	-0.042537	3.929370
209.926218	5257.031640	7.564352	-0.042613	3.932261
210.211337	5265.078519	7.569357	-0.042671	3.935151
210.465029	5273.137335	7.574362	-0.042724	3.938042
210.633457	5281.095537	7.579366	-0.042760	3.940894
210.753734	5289.113421	7.584371	-0.042788	3.943765
211.080079	5297.133394	7.589376	-0.042854	3.946637
211.278358	5305.133151	7.594381	-0.042896	3.949498
211.451627	5313.250241	7.599386	-0.042934	3.952399
211.676298	5321.262355	7.604390	-0.042981	3.955260
212.003686	5329.253603	7.609395	-0.043047	3.958114
212.135531	5337.237192	7.614400	-0.043077	3.960960
212.276667	5345.193681	7.619405	-0.043109	3.963794
212.693607	5353.258064	7.624410	-0.043192	3.966669
212.661366	5361.265928	7.629414	-0.043191	3.969514
212.876967	5369.324315	7.634419	-0.043237	3.972380
213.134553	5377.370840	7.639424	-0.043290	3.975239
213.279067	5385.350096	7.644429	-0.043322	3.978071
213.453154	5393.368123	7.649434	-0.043360	3.980916
213.598719	5401.361517	7.654438	-0.043392	3.983749
213.751404	5409.408888	7.659443	-0.043426	3.986599
213.964842	5417.411650	7.664448	-0.043471	3.989432
214.016824	5425.450448	7.669453	-0.043486	3.992273
214.399327	5433.511144	7.674458	-0.043562	3.995125
214.366464	5441.509566	7.679462	-0.043562	3.997947
214.476538	5449.545369	7.684467	-0.043587	4.000782
214.769473	5457.530084	7.689472	-0.043647	4.003600
214.828153	5465.556597	7.694477	-0.043664	4.006427
215.026102	5473.620875	7.699482	-0.043706	4.009267
215.173756	5481.630978	7.704486	-0.043738	4.012086
215.388581	5489.649199	7.709491	-0.043784	4.014906
215.466090	5497.685323	7.714496	-0.043804	4.017729
215.657963	5505.674146	7.719501	-0.043845	4.020535
215.934034	5513.701550	7.724506	-0.043901	4.023353
216.104723	5521.709787	7.729510	-0.043938	4.026162
216.224619	5529.739233	7.734515	-0.043966	4.028974
216.519150	5537.776786	7.739520	-0.044026	4.031791
216.650710	5545.871614	7.744525	-0.044056	4.034623
216.884653	5553.876723	7.749530	-0.044105	4.037423
217.012452	5561.818566	7.754534	-0.044134	4.040197
217.438569	5569.828748	7.759539	-0.044219	4.042998
217.453339	5577.848219	7.764544	-0.044227	4.045794
217.718674	5585.828890	7.769549	-0.044281	4.048578
218.194201	5593.898974	7.774554	-0.044375	4.051395
218.041249	5601.903512	7.779558	-0.044352	4.054177
218.215699	5609.945146	7.784563	-0.044390	4.056976
218.273914	5617.917095	7.789568	-0.044406	4.059746
218.363543	5625.956228	7.794573	-0.044428	4.062538
218.773237	5633.927850	7.799578	-0.044509	4.065310
218.969854	5641.968503	7.804582	-0.044551	4.068100
219.386613	5649.957390	7.809587	-0.044634	4.070874
219.523890	5658.013413	7.814592	-0.044665	4.073665
219.666443	5666.073917	7.819597	-0.044697	4.076456
220.019943	5674.074893	7.824602	-0.044768	4.079227
220.178734	5682.084489	7.829606	-0.044803	4.081996
220.251856	5690.064005	7.834611	-0.044822	4.084752
220.316576	5698.109009	7.839616	-0.044839	4.087529
220.550759	5706.097803	7.844621	-0.044888	4.090287
220.757499	5714.172896	7.849626	-0.044932	4.093072
220.832615	5722.174202	7.854630	-0.044951	4.095828
221.151714	5730.183572	7.859635	-0.045016	4.098588
221.104451	5738.216712	7.864640	-0.045012	4.101350
221.249549	5746.216295	7.869645	-0.045045	4.104101
221.827064	5754.271717	7.874650	-0.045158	4.106874
221.798922	5762.238617	7.879654	-0.045158	4.109608
222.092337	5770.332926	7.884659	-0.045218	4.112388
222.174485	5778.368534	7.889664	-0.045238	4.115142
222.504911	5786.367757	7.894669	-0.045305	4.117886
222.582159	5794.358758	7.899674	-0.045325	4.120622
222.693649	5802.342012	7.904678	-0.045351	4.123354
222.821483	5810.401305	7.909683	-0.045380	4.126110
223.032847	5818.412801	7.914688	-0.045425	4.128849
223.180450	5826.430126	7.919693	-0.045457	4.131587
223.395156	5834.497186	7.924698	-0.045503	4.134341
223.724743	5842.518998	7.929702	-0.045569	4.137079
223.997249	5850.524407	7.934707	-0.045625	4.139810
224.023963	5858.544598	7.939712	-0.045636	4.142540
224.238686	5866.464519	7.944717	-0.045681	4.145237
224.545776	5874.566604	7.949722	-0.045743	4.147995
224.510905	5882.584665	7.954726	-0.045742	4.150719
224.657739	5890.649709	7.959731	-0.045775	4.153458
224.868134	5898.653589	7.964736	-0.045819	4.156176
225.020109	5906.626980	7.969741	-0.045853	4.158882
225.286326	5914.655316	7.974746	-0.045908	4.161605
225.639531	5922.605933	7.979750	-0.045979	4.164301
225.760803	5930.698633	7.984755	-0.046007	4.167041
225.926166	5938.671537	7.989760	-0.046043	4.169739
226.195586	5946.712860	7.994765	-0.046098	4.172460
226.339495	5954.797789	7.999770	-0.046130	4.175192
226.289605	5962.773038	8.004774	-0.046126	4.177883
226.683104	5970.753266	8.009779	-0.046205	4.180579
226.941257	5978.780134	8.014784	-0.046258	4.183287
227.016596	5986.747573	8.019789	-0.046278	4.185972
227.203389	5994.802981	8.024794	-0.046318	4.188685
227.371446	6002.844782	8.029798	-0.046354	4.191392
227.678853	6010.938676	8.034803	-0.046417	4.194117
227.796760	6018.982393	8.039808	-0.046444	4.196820
228.145490	6026.864376	8.044813	-0.046514	4.199470
228.262554	6034.946470	8.049818	-0.046542	4.202183
228.201428	6042.898537	8.054822	-0.046535	4.204849
228.320807	6050.903391	8.059827	-0.046563	4.207533
228.549170	6058.915793	8.064832	-0.046611	4.210218
228.647100	6066.970829	8.069837	-0.046634	4.212915
229.008031	6075.004742	8.074842	-0.046707	4.215606
229.187392	6083.012755	8.079846	-0.046746	4.218284
229.420101	6090.981399	8.084851	-0.046794	4.220948
229.415522	6099.079827	8.089856	-0.046799	4.223651
229.539483	6107.040323	8.094861	-0.046827	4.226308
229.832773	6115.073252	8.099866	-0.046887	4.228989
229.925935	6123.090751	8.104870	-0.046910	4.231661
229.974413	6131.172755	8.109875	-0.046924	4.234353
230.256432	6139.192493	8.114880	-0.046982	4.237024
230.468723	6147.088783	8.119885	-0.047027	4.239652
230.366308	6155.220382	8.124890	-0.047013	4.242353
230.633639	6163.080116	8.129894	-0.047068	4.244966
230.911489	6171.227737	8.134899	-0.047125	4.247673
230.996937	6179.189013	8.139904	-0.047146	4.250314
231.317387	6187.268736	8.144909	-0.047211	4.252995
231.798351	6195.252399	8.149914	-0.047306	4.255644
231.825237	6203.305856	8.154918	-0.047316	4.258311
232.125308	6211.272390	8.159923	-0.047377	4.260949
232.358030	6219.349607	8.164928	-0.047426	4.263622
232.549272	6227.294122	8.169933	-0.047467	4.266249
232.796440	6235.383115	8.174938	-0.047518	4.268922
233.047609	6243.384453	8.179942	-0.047570	4.271565
233.078307	6251.493848	8.184947	-0.047581	4.274240
233.375096	6259.470105	8.189952	-0.047642	4.276871
233.584414	6267.429835	8.194957	-0.047686	4.279495
233.836475	6275.505447	8.199962	-0.047739	4.282156
233.929323	6283.425798	8.204966	-0.047761	4.284762
234.070794	6291.488530	8.209971	-0.047793	4.287414
234.390950	6299.495079	8.214976	-0.047858	4.290048
234.606809	6307.562382	8.219981	-0.047903	4.292699
234.768976	6315.602709	8.224986	-0.047939	4.295339
235.187462	6323.577409	8.229990	-0.048022	4.297957
235.280514	6331.566482	8.234995	-0.048044	4.300577
235.382831	6339.603163	8.240000	-0.048069	4.303210
235.627415	6347.592020	8.245005	-0.048120	4.305827
235.878467	6355.626746	8.250010	-0.048172	4.308458
235.915883	6363.673109	8.255014	-0.048184	4.311089
236.113833	6371.692235	8.260019	-0.048226	4.313711
236.485228	6379.715443	8.265024	-0.048301	4.316334
236.634641	6387.687211	8.270029	-0.048334	4.318937
236.621664	6395.707518	8.275034	-0.048337	4.321553
237.000877	6403.689943	8.280038	-0.048413	4.324157
236.988815	6411.733432	8.285043	-0.048416	4.326778
237.213149	6419.744304	8.290048	-0.048463	4.329387
237.441438	6427.770584	8.295053	-0.048510	4.332000
237.732908	6435.829343	8.300058	-0.048570	4.334623
237.681233	6443.865399	8.305062	-0.048566	4.337234
237.886435	6451.818489	8.310067	-0.048609	4.339819
238.292459	6459.828261	8.315072	-0.048690	4.342421
238.249456	6467.796883	8.320077	-0.048687	4.345006
238.473637	6475.881644	8.325082	-0.048734	4.347628
238.726035	6483.890847	8.330086	-0.048787	4.350225
238.886326	6491.943333	8.335091	-0.048822	4.352833
239.073618	6500.035924	8.340096	-0.048862	4.355453
239.128176	6507.997844	8.345101	-0.048878	4.358029
239.533606	6515.989966	8.350106	-0.048958	4.360614
239.639344	6523.962459	8.355110	-0.048983	4.363190
239.889436	6531.971952	8.360115	-0.049035	4.365777
240.197374	6539.981409	8.365120	-0.049098	4.368363
240.247233	6547.990579	8.370125	-0.049112	4.370946
240.388750	6556.055258	8.375130	-0.049144	4.373546
240.559428	6564.081635	8.380134	-0.049181	4.376132
240.828596	6572.097587	8.385139	-0.049237	4.378713
240.940286	6580.098691	8.390144	-0.049263	4.381288
241.084899	6588.071953	8.395149	-0.049295	4.383852
241.471134	6596.144171	8.400154	-0.049372	4.386448
241.640440	6604.106184	8.405158	-0.049409	4.389005
241.732801	6612.180213	8.410163	-0.049431	4.391597
242.037396	6620.216767	8.415168	-0.049494	4.394176
242.269948	6628.207657	8.420173	-0.049542	4.396738
242.319241	6636.213922	8.425178	-0.049557	4.399303
242.234074	6644.208392	8.430182	-0.049546	4.401862
242.508513	6652.207964	8.435187	-0.049602	4.404423
242.595204	6660.285394	8.440192	-0.049624	4.407007
242.823568	6668.237538	8.445197	-0.049672	4.409549
243.233121	6676.316914	8.450202	-0.049753	4.412132
243.431426	6684.331797	8.455206	-0.049795	4.414691
243.517531	6692.397035	8.460211	-0.049817	4.417265
243.902844	6700.343406	8.465216	-0.049894	4.419800
244.125537	6708.419211	8.470221	-0.049941	4.422375
244.299918	6716.390639	8.475226	-0.049978	4.424914
244.364895	6724.436848	8.480230	-0.049996	4.427475
244.485399	6732.427144	8.485235	-0.050024	4.430018
244.763777	6740.543835	8.490240	-0.050081	4.432599
244.869956	6748.502424	8.495245	-0.050106	4.435128
245.068418	6756.554938	8.500250	-0.050148	4.437686
245.155378	6764.503337	8.505254	-0.050169	4.440209
245.425342	6772.501361	8.510259	-0.050225	4.442747
245.565658	6780.489842	8.515264	-0.050256	4.445280
245.761242	6788.556230	8.520269	-0.050298	4.447836
246.193459	6796.567439	8.525274	-0.050384	4.450374
246.308751	6804.624458	8.530278	-0.050411	4.452924
246.496827	6812.642888	8.535283	-0.050451	4.455461
246.796220	6820.645994	8.540288	-0.050512	4.457992
246.846795	6828.593152	8.545293	-0.050527	4.460502
246.935002	6836.678943	8.550298	-0.050549	4.463056
247.182719	6844.641094	8.555302	-0.050600	4.465569
247.384999	6852.695435	8.560307	-0.050643	4.468109
247.414453	6860.688775	8.565312	-0.050654	4.470629
247.812466	6868.696967	8.570317	-0.050733	4.473153
247.987761	6876.766510	8.575322	-0.050771	4.475694
248.115819	6884.776641	8.580327	-0.050800	4.478214
248.397499	6892.743277	8.585331	-0.050858	4.480720
248.685019	6900.778035	8.590336	-0.050917	4.483246
248.727850	6908.766873	8.595341	-0.050930	4.485756
248.837108	6916.796453	8.600346	-0.050956	4.488277
249.136351	6924.820070	8.605351	-0.051017	4.490795
249.422468	6932.851411	8.610355	-0.051075	4.493314
249.387049	6940.898883	8.615360	-0.051074	4.495836
249.559476	6948.859538	8.620365	-0.051111	4.498330
249.793619	6956.905029	8.625370	-0.051160	4.500849
249.989697	6964.897513	8.630375	-0.051202	4.503350
250.150763	6972.900767	8.635379	-0.051237	4.505853
250.542704	6980.951917	8.640384	-0.051316	4.508370
250.571788	6988.931175	8.645389	-0.051326	4.510862
250.849204	6997.068311	8.650394	-0.051383	4.513403
250.983209	7005.055905	8.655399	-0.051414	4.515895
251.366492	7013.028423	8.660403	-0.051490	4.518382
251.354371	7021.013843	8.665408	-0.051493	4.520871
251.459044	7028.990966	8.670413	-0.051518	4.523355
251.650912	7037.041263	8.675418	-0.051559	4.525862
251.660187	7045.028824	8.680423	-0.051566	4.528347
251.761205	7053.032365	8.685427	-0.051590	4.530836
252.072370	7061.085542	8.690432	-0.051654	4.533339
252.216835	7069.093820	8.695437	-0.051686	4.535827
252.735834	7077.146105	8.700442	-0.051788	4.538327
252.796410	7085.117465	8.705447	-0.051804	4.540800
253.067961	7093.148725	8.710451	-0.051860	4.543291
253.248503	7101.178822	8.715456	-0.051899	4.545780
253.497577	7109.179871	8.720461	-0.051951	4.548258
253.853041	7117.196109	8.725466	-0.052022	4.550740
253.933188	7125.242019	8.730471	-0.052042	4.553230
254.247183	7133.287594	8.735475	-0.052106	4.555718
254.313848	7141.292963	8.740480	-0.052124	4.558192
254.435799	7149.221683	8.745485	-0.052152	4.560642
254.679808	7157.300070	8.750490	-0.052203	4.563136
254.892524	7165.254517	8.755495	-0.052248	4.565590
255.240872	7173.298105	8.760499	-0.052318	4.568071
255.338563	7181.309218	8.765504	-0.052341	4.570540
255.450352	7189.364221	8.770509	-0.052367	4.573022
255.692742	7197.396057	8.775514	-0.052418	4.575494
255.700464	7205.393088	8.780519	-0.052425	4.577955
255.987101	7213.403239	8.785523	-0.052483	4.580419
256.231435	7221.463585	8.790528	-0.052534	4.582896
256.351900	7229.397363	8.795533	-0.052562	4.585334
256.863521	7237.529444	8.800538	-0.052662	4.587831
256.807701	7245.492379	8.805543	-0.052657	4.590274
257.107920	7253.521578	8.810547	-0.052718	4.592737
257.118491	7261.542990	8.815552	-0.052726	4.595196
257.332704	7269.578942	8.820557	-0.052771	4.597658
257.619544	7277.568330	8.825562	-0.052830	4.600104
257.867077	7285.597782	8.830567	-0.052881	4.602562
257.809781	7293.533384	8.835571	-0.052876	4.604989
258.067530	7301.608299	8.840576	-0.052929	4.607458
258.404699	7309.544662	8.845581	-0.052997	4.609882
258.472055	7317.659837	8.850586	-0.053015	4.612361
258.454059	7325.676964	8.855591	-0.053017	4.614808
258.764420	7333.697902	8.860595	-0.053080	4.617254
258.950344	7341.687132	8.865600	-0.053120	4.619690
258.922610	7349.694547	8.870605	-0.053120	4.622130
259.268317	7357.691687	8.875610	-0.053190	4.624566
259.507282	7365.721638	8.880615	-0.053239	4.627010
259.577335	7373.694916	8.885619	-0.053258	4.629436
259.873091	7381.771662	8.890624	-0.053318	4.631892
260.015969	7389.791717	8.895629	-0.053350	4.634329
260.160306	7397.814006	8.900634	-0.053382	4.636766
260.226427	7405.787846	8.905639	-0.053400	4.639186
260.396076	7413.794056	8.910643	-0.053437	4.641616
260.553936	7421.807577	8.915648	-0.053471	4.644046
260.442332	7429.772747	8.920653	-0.053456	4.646460
260.781698	7437.792412	8.925658	-0.053524	4.648890
260.880309	7445.899896	8.930663	-0.053548	4.651344
260.936932	7453.892848	8.935667	-0.053564	4.653763
261.274693	7461.922339	8.940672	-0.053632	4.656192
261.285210	7469.914209	8.945677	-0.053639	4.658608
261.500468	7477.943361	8.950682	-0.053685	4.661034
261.727018	7485.919979	8.955687	-0.053732	4.663442
261.991031	7493.896891	8.960691	-0.053787	4.665850
262.159711	7501.977879	8.965696	-0.053823	4.668287
262.501590	7509.953402	8.970701	-0.053892	4.670692
262.833366	7518.090616	8.975706	-0.053960	4.673143
262.844233	7526.102642	8.980711	-0.053967	4.675557
263.037642	7534.086845	8.985715	-0.054008	4.677960
263.194766	7542.100934	8.990720	-0.054043	4.680371
263.297252	7550.036808	8.995725	-0.054067	4.682757
263.529103	7558.048361	9.000730	-0.054115	4.685165
263.596556	7566.090973	9.005735	-0.054133	4.687581
263.696153	7574.066256	9.010739	-0.054157	4.689976
263.777105	7582.144364	9.015744	-0.054178	4.692400
263.775922	7590.103185	9.020749	-0.054183	4.694787
264.353240	7598.192698	9.025754	-0.054295	4.697211
264.425304	7606.122912	9.030759	-0.054314	4.699588
264.595627	7614.213381	9.035763	-0.054351	4.702010
264.870588	7622.198441	9.040768	-0.054408	4.704400
265.051587	7630.150296	9.045773	-0.054447	4.706778
265.332073	7638.226218	9.050778	-0.054504	4.709193
265.498718	7646.244729	9.055783	-0.054541	4.711589
265.627845	7654.226264	9.060787	-0.054570	4.713973
266.039966	7662.312991	9.065792	-0.054652	4.716386
265.994737	7670.281200	9.070797	-0.054649	4.718764
266.370449	7678.298549	9.075802	-0.054724	4.721154
266.241427	7686.359904	9.080807	-0.054705	4.723558
266.379024	7694.279330	9.085811	-0.054736	4.725917
266.493258	7702.354564	9.090816	-0.054763	4.728322
266.808960	7710.376377	9.095821	-0.054827	4.730709
267.076073	7718.448012	9.100826	-0.054882	4.733109
267.076448	7726.441006	9.105831	-0.054887	4.735486
267.338003	7734.446302	9.110835	-0.054941	4.737864
267.476345	7742.430100	9.115840	-0.054972	4.740235
267.512988	7750.465121	9.120845	-0.054985	4.742621
267.675736	7758.459443	9.125850	-0.055020	4.744993
267.973916	7766.517417	9.130855	-0.055081	4.747382
268.234982	7774.505372	9.135859	-0.055135	4.749749
268.339617	7782.553388	9.140864	-0.055160	4.752133
268.461519	7790.578303	9.145869	-0.055188	4.754509
268.592253	7798.579975	9.150874	-0.055217	4.756877
268.709693	7806.569682	9.155879	-0.055244	4.759241
269.062917	7814.597234	9.160883	-0.055316	4.761613
269.328779	7822.554830	9.165888	-0.055370	4.763964
269.365334	7830.577752	9.170893	-0.055382	4.766334
269.583099	7838.624174	9.175898	-0.055428	4.768709
269.844310	7846.653102	9.180903	-0.055482	4.771077
269.877109	7854.656340	9.185907	-0.055494	4.773438
270.071515	7862.699837	9.190912	-0.055535	4.775808
270.298041	7870.675829	9.195917	-0.055583	4.778157
270.345928	7878.679648	9.200922	-0.055597	4.780515
270.345069	7886.725946	9.205927	-0.055602	4.782883
270.773739	7894.657668	9.210931	-0.055687	4.785215
271.062804	7902.767507	9.215936	-0.055746	4.787599
271.024662	7910.709506	9.220941	-0.055744	4.789933
271.292834	7918.800611	9.225946	-0.055800	4.792309
271.401832	7926.814553	9.230951	-0.055825	4.794662
271.457791	7934.847566	9.235955	-0.055841	4.797019
271.764052	7942.797192	9.240960	-0.055903	4.799350
271.800803	7950.846367	9.245965	-0.055915	4.801710
271.996104	7958.769040	9.250970	-0.055957	4.804031
272.007200	7966.797984	9.255975	-0.055964	4.806383
272.318395	7974.872383	9.260979	-0.056028	4.808745
272.515148	7982.896569	9.265984	-0.056070	4.811092
272.562653	7990.410690	9.270989	-0.056083	4.813290
272.748981	7995.185946	9.275994	-0.056121	4.814685

272.849056	7997.762759	9.280999	-0.056142	4.815438
273.017101	7999.093516	9.286003	-0.056174	4.815826
273.118256	7999.602756	9.291008	-0.056193	4.815974
273.233438	8000.363313	9.296013	-0.056215	4.816196
273.389683	8000.649250	9.301018	-0.056245	4.816278
273.292291	8000.534253	9.306023	-0.056226	4.816245
273.463936	8000.552326	9.311027	-0.056259	4.816250
273.580687	8000.535219	9.316032	-0.056280	4.816244
273.600361	8000.611433	9.321037	-0.056284	4.816266
273.656998	8000.583623	9.326042	-0.056295	4.816258
273.665134	8000.617964	9.331047	-0.056296	4.816268
273.787622	8000.533657	9.336051	-0.056319	4.816242
273.627433	8000.508328	9.341056	-0.056289	4.816236
273.636681	8000.532006	9.346061	-0.056291	4.816243
274.023333	8000.550771	9.351066	-0.056363	4.816246
273.886399	8000.527999	9.356071	-0.056338	4.816240
273.968298	8000.610683	9.361075	-0.056353	4.816264
274.031937	8000.528515	9.366080	-0.056365	4.816240
273.850450	8000.614972	9.371085	-0.056331	4.816266
274.067968	8000.520636	9.376090	-0.056372	4.816237
274.002368	8000.529070	9.381095	-0.056360	4.816240
274.049511	8000.564118	9.386099	-0.056369	4.816250
274.185472	8000.560180	9.391104	-0.056394	4.816248
274.038625	8000.562867	9.396109	-0.056367	4.816250
274.319677	8000.460068	9.401114	-0.056419	4.816218
274.400831	8000.545944	9.406119	-0.056434	4.816243
274.274882	8000.603495	9.411123	-0.056411	4.816260
274.343910	8000.456256	9.416128	-0.056424	4.816217
274.324891	8000.584118	9.421133	-0.056421	4.816254
274.371016	8000.528340	9.426138	-0.056429	4.816238
274.392419	8000.627022	9.431143	-0.056433	4.816266
274.346938	8000.643298	9.436147	-0.056425	4.816271
274.379530	8000.456939	9.441152	-0.056431	4.816217
274.456953	8000.598301	9.446157	-0.056446	4.816258
274.625958	8000.472104	9.451162	-0.056477	4.816220
274.559386	8000.571328	9.456167	-0.056465	4.816249
274.704362	8000.469267	9.461171	-0.056492	4.816219
274.812093	8000.424220	9.466176	-0.056512	4.816205
275.024672	8000.565896	9.471181	-0.056552	4.816245
274.879255	8000.534423	9.476186	-0.056525	4.816237
274.783895	8000.639536	9.481191	-0.056507	4.816268
274.740794	8000.440051	9.486195	-0.056499	4.816210
274.757759	8000.534380	9.491200	-0.056502	4.816237
274.765386	8000.549482	9.496205	-0.056504	4.816242
275.142408	8000.430260	9.501210	-0.056574	4.816205
275.108326	8000.520459	9.506215	-0.056568	4.816232
274.736985	8000.493436	9.511219	-0.056499	4.816226
275.017585	8000.512419	9.516224	-0.056551	4.816230
274.939583	8000.613573	9.521229	-0.056537	4.816260
274.961198	8000.456926	9.526234	-0.056541	4.816214
275.228637	8000.516267	9.531239	-0.056590	4.816230
275.373601	8000.402453	9.536243	-0.056617	4.816196
275.418155	8000.428909	9.541248	-0.056626	4.816203
275.148752	8000.438989	9.546253	-0.056576	4.816207
275.198174	8000.436688	9.551258	-0.056585	4.816207
275.451152	8000.488289	9.556263	-0.056632	4.816220
275.104779	8000.453172	9.561267	-0.056568	4.816212
275.175054	8000.518554	9.566272	-0.056581	4.816231
275.135224	8000.439850	9.571277	-0.056574	4.816208
275.247338	8000.549793	9.576282	-0.056595	4.816239
275.261855	8000.527628	9.581287	-0.056597	4.816233
275.393437	8000.539637	9.586291	-0.056622	4.816236
275.427593	8000.280656	9.591296	-0.056628	4.816160
275.350235	8000.437375	9.596301	-0.056614	4.816206
275.576473	8000.426527	9.601306	-0.056656	4.816202
275.409050	8000.312392	9.606311	-0.056625	4.816169
275.374041	8000.488042	9.611315	-0.056619	4.816221
275.534742	8000.436477	9.616320	-0.056649	4.816205
275.676818	8000.549101	9.621325	-0.056675	4.816237
275.696282	8000.445831	9.626330	-0.056679	4.816207
275.496346	8000.414437	9.631335	-0.056642	4.816198
275.757433	8000.529218	9.636339	-0.056691	4.816231
275.686126	8000.476652	9.641344	-0.056677	4.816216
275.661157	8000.575564	9.646349	-0.056673	4.816245
275.770063	8000.337166	9.651354	-0.056693	4.816174
275.682088	8000.376176	9.656359	-0.056677	4.816186
275.664720	8000.436765	9.661363	-0.056674	4.816204
275.879363	8000.295368	9.666368	-0.056714	4.816162
275.711395	8000.501727	9.671373	-0.056683	4.816223
275.658230	8000.243299	9.676378	-0.056673	4.816148
275.492069	8000.434733	9.681383	-0.056642	4.816204
275.765308	8000.476018	9.686387	-0.056693	4.816215
275.670854	8000.479655	9.691392	-0.056675	4.816217
275.368937	8000.430387	9.696397	-0.056619	4.816204
275.534324	8000.432324	9.701402	-0.056650	4.816203
275.635114	8000.424544	9.706407	-0.056669	4.816201
275.647640	8000.379908	9.711411	-0.056671	4.816187
275.709528	8000.281681	9.716416	-0.056683	4.816158
275.895577	8000.458134	9.721421	-0.056718	4.816209
275.899802	8000.374887	9.726426	-0.056718	4.816185
275.637162	8000.428892	9.731431	-0.056670	4.816202
275.654542	8000.561691	9.736435	-0.056673	4.816241
275.722948	8000.292645	9.741440	-0.056686	4.816162
275.653831	8000.564898	9.746445	-0.056673	4.816242
275.633558	8000.467317	9.751450	-0.056669	4.816213
275.994171	8000.523008	9.756455	-0.056737	4.816227
275.867106	8000.472635	9.761459	-0.056713	4.816213
275.921298	8000.207606	9.766464	-0.056723	4.816136
275.820135	8000.578635	9.771469	-0.056704	4.816245
275.910963	8000.557854	9.776474	-0.056721	4.816238
275.850328	8000.360184	9.781479	-0.056710	4.816181
275.894609	8000.449668	9.786483	-0.056718	4.816207
275.998976	8000.355416	9.791488	-0.056738	4.816178
275.969049	8000.561074	9.796493	-0.056732	4.816239
276.112022	8000.409830	9.801498	-0.056759	4.816194
275.831479	8000.444280	9.806503	-0.056707	4.816205
275.833668	8000.433644	9.811507	-0.056707	4.816202
275.866871	8000.476987	9.816512	-0.056714	4.816215
276.020372	8000.536402	9.821517	-0.056742	4.816231
275.979969	8000.389311	9.826522	-0.056735	4.816188
275.742373	8000.458727	9.831527	-0.056691	4.816210
275.802809	8000.430985	9.836531	-0.056702	4.816202
276.138482	8000.508660	9.841536	-0.056765	4.816222
275.999999	8000.479447	9.846541	-0.056739	4.816215
276.002461	8000.488046	9.851546	-0.056740	4.816217
276.300430	8000.372732	9.856551	-0.056795	4.816182
276.299749	8000.366317	9.861555	-0.056795	4.816180
276.102754	8000.422580	9.866560	-0.056758	4.816197
276.132992	8000.466939	9.871565	-0.056764	4.816210
276.312667	8000.278968	9.876570	-0.056798	4.816154
276.228356	8000.423812	9.881575	-0.056782	4.816197
276.136125	8000.570650	9.886579	-0.056765	4.816241
276.347554	8000.434536	9.891584	-0.056804	4.816200
276.227368	8000.552021	9.896589	-0.056782	4.816235
276.050492	8000.429164	9.901594	-0.056749	4.816200
275.964399	8000.461798	9.906599	-0.056733	4.816210
275.969028	8000.382831	9.911603	-0.056734	4.816187
275.946592	8000.454011	9.916608	-0.056730	4.816207
275.997557	8000.594899	9.921613	-0.056740	4.816248
276.069055	8000.467999	9.926618	-0.056753	4.816211
276.134471	8000.431800	9.931623	-0.056765	4.816200
276.075870	8000.469206	9.936627	-0.056754	4.816211
276.229050	8000.635453	9.941632	-0.056783	4.816259
276.106775	8000.541362	9.946637	-0.056760	4.816232
276.075331	8000.439305	9.951642	-0.056755	4.816202
276.130898	8000.567456	9.956647	-0.056765	4.816240
276.361841	8000.559900	9.961651	-0.056808	4.816236
276.188160	8000.317443	9.966656	-0.056776	4.816166
276.287959	8000.637635	9.971661	-0.056795	4.816259
276.262110	8000.538883	9.976666	-0.056790	4.816231
276.274733	8000.548735	9.981671	-0.056792	4.816233
276.243413	8000.448816	9.986675	-0.056786	4.816204
276.293115	8000.388828	9.991680	-0.056796	4.816187
276.348604	8000.591764	9.996685	-0.056806	4.816246
276.433066	8000.451209	10.001690	-0.056822	4.816204
276.439529	8000.424625	10.006695	-0.056823	4.816196
276.345704	8000.465666	10.011699	-0.056806	4.816209
276.275796	8000.297740	10.016704	-0.056793	4.816160
276.227067	8000.545794	10.021709	-0.056784	4.816233
276.270864	8000.429075	10.026714	-0.056792	4.816198
276.274951	8000.437703	10.031719	-0.056793	4.816201
276.293076	8000.574791	10.036723	-0.056797	4.816241
276.345918	8000.456099	10.041728	-0.056806	4.816206
276.438849	8000.567835	10.046733	-0.056824	4.816238
276.269895	8000.397044	10.051738	-0.056792	4.816189
276.453455	8000.491192	10.056743	-0.056827	4.816216
276.444264	8000.319025	10.061747	-0.056825	4.816165
276.451588	8000.360832	10.066752	-0.056826	4.816178
276.186590	8000.534451	10.071757	-0.056777	4.816230
276.485285	8000.548424	10.076762	-0.056833	4.816232
276.262078	8000.391606	10.081767	-0.056791	4.816187
276.248781	8000.508892	10.086771	-0.056789	4.816222
276.360951	8000.341064	10.091776	-0.056810	4.816172
276.302178	8000.569705	10.096781	-0.056799	4.816239
276.392327	8000.226265	10.101786	-0.056816	4.816138
276.603031	8000.409579	10.106791	-0.056855	4.816191
276.516961	8000.473196	10.111795	-0.056839	4.816210
276.484301	8000.321971	10.116800	-0.056833	4.816166
276.387373	8000.425989	10.121805	-0.056815	4.816197
276.664711	8000.576326	10.126810	-0.056867	4.816239
276.598066	8000.456535	10.131815	-0.056855	4.816205
276.509072	8000.524373	10.136819	-0.056838	4.816225
276.480963	8000.352931	10.141824	-0.056833	4.816175
276.513174	8000.514847	10.146829	-0.056839	4.816222
276.347973	8000.214852	10.151834	-0.056808	4.816135
276.415640	8000.366726	10.156839	-0.056821	4.816179
276.465436	8000.354816	10.161843	-0.056830	4.816176
276.401419	8000.285287	10.166848	-0.056819	4.816156
276.481132	8000.378620	10.171853	-0.056834	4.816182
276.577180	8000.348318	10.176858	-0.056851	4.816173
276.582531	8000.227697	10.181863	-0.056852	4.816138
276.410420	8000.472445	10.186867	-0.056821	4.816210
276.721920	8000.278316	10.191872	-0.056879	4.816152
276.861964	8000.387701	10.196877	-0.056905	4.816183
276.645718	8000.195754	10.201882	-0.056865	4.816128
276.750210	8000.380347	10.206887	-0.056884	4.816182
276.778121	8000.565691	10.211891	-0.056890	4.816236
276.586543	8000.077184	10.216896	-0.056854	4.816094
276.603295	8000.202493	10.221901	-0.056857	4.816130
276.850138	8000.045654	10.226906	-0.056903	4.816083
276.587970	8000.286631	10.231911	-0.056854	4.816155
276.471717	8000.320855	10.236915	-0.056833	4.816166
276.616831	8000.291443	10.241920	-0.056860	4.816156
276.495687	8000.375791	10.246925	-0.056837	4.816182
276.623197	8000.211446	10.251930	-0.056861	4.816133
276.493385	8000.137520	10.256935	-0.056837	4.816112
276.461822	8000.308961	10.261939	-0.056831	4.816162
276.771912	8000.076346	10.266944	-0.056889	4.816093
276.787912	8000.506130	10.271949	-0.056892	4.816218
276.903929	8000.391788	10.276954	-0.056914	4.816184
276.776841	8000.220687	10.281959	-0.056890	4.816135
276.627461	8000.415635	10.286963	-0.056863	4.816192
276.840316	8000.246426	10.291968	-0.056902	4.816142
276.797396	8000.571511	10.296973	-0.056894	4.816237
276.776568	8000.273063	10.301978	-0.056890	4.816150
276.776696	8000.267731	10.306983	-0.056891	4.816148
276.891434	8000.443965	10.311987	-0.056912	4.816199
276.808259	8000.114473	10.316992	-0.056897	4.816104
276.764302	8000.413896	10.321997	-0.056889	4.816191
276.911698	8000.129184	10.327002	-0.056916	4.816107
276.951036	8000.463239	10.332007	-0.056924	4.816205
276.814824	8000.406288	10.337011	-0.056898	4.816189
276.881835	8000.393622	10.342016	-0.056911	4.816185
276.776061	8000.570131	10.347021	-0.056891	4.816237
276.821272	8000.416043	10.352026	-0.056900	4.816192
276.739217	8000.357938	10.357031	-0.056884	4.816175
276.976544	8000.427421	10.362035	-0.056929	4.816194
277.110673	7999.943752	10.367040	-0.056953	4.816052
276.939128	8000.371202	10.372045	-0.056922	4.816178
276.974399	8000.265011	10.377050	-0.056928	4.816147
276.988864	8000.317632	10.382055	-0.056931	4.816162
277.119350	8000.567872	10.387059	-0.056956	4.816234
277.023162	7999.959297	10.392064	-0.056938	4.816057
276.927066	8000.215038	10.397069	-0.056920	4.816132
277.098800	8000.125211	10.402074	-0.056952	4.816105
276.911479	8000.074814	10.407079	-0.056917	4.816091
276.935393	8000.249399	10.412083	-0.056922	4.816142
276.916996	8000.229842	10.417088	-0.056918	4.816137
277.030117	8000.493655	10.422093	-0.056940	4.816213
276.876600	8000.141519	10.427098	-0.056911	4.816111
276.869396	8000.015329	10.432103	-0.056910	4.816074
276.860647	8000.248081	10.437107	-0.056908	4.816142
277.095006	8000.267296	10.442112	-0.056952	4.816147
276.997252	8000.398010	10.447117	-0.056934	4.816185
276.993924	8000.062488	10.452122	-0.056933	4.816087
276.941478	8000.092527	10.457127	-0.056923	4.816096
276.898101	8000.271234	10.462131	-0.056916	4.816149
277.119623	8000.020987	10.467136	-0.056957	4.816074
276.960700	8000.300162	10.472141	-0.056927	4.816157
277.035832	8000.055807	10.477146	-0.056941	4.816085
277.021745	8000.047012	10.482151	-0.056939	4.816083
277.163219	8000.152148	10.487155	-0.056965	4.816113
276.923059	8000.040965	10.492160	-0.056921	4.816081
276.761457	8000.449364	10.497165	-0.056891	4.816202
276.984936	8000.305989	10.502170	-0.056932	4.816158
277.246787	8000.367370	10.507175	-0.056981	4.816175
277.124842	8000.358756	10.512179	-0.056959	4.816173
277.196900	8000.034215	10.517184	-0.056972	4.816078
277.193931	8000.509599	10.522189	-0.056972	4.816217
277.182112	8000.287167	10.527194	-0.056969	4.816152
277.333408	8000.205516	10.532199	-0.056998	4.816127
277.122908	8000.452776	10.537203	-0.056959	4.816201
277.242664	8000.392990	10.542208	-0.056981	4.816182
277.195667	8000.415649	10.547213	-0.056972	4.816189
277.290566	8000.115026	10.552218	-0.056990	4.816101
277.277666	8000.291082	10.557223	-0.056988	4.816153
277.047966	8000.200385	10.562227	-0.056945	4.816127
277.267240	8000.322960	10.567232	-0.056986	4.816162
277.263450	8000.546193	10.572237	-0.056985	4.816227
277.142810	8000.456403	10.577242	-0.056963	4.816202
277.092179	8000.252499	10.582247	-0.056954	4.816142
277.119974	8000.366259	10.587251	-0.056959	4.816175
277.299189	8000.227422	10.592256	-0.056992	4.816134
277.248177	8000.439113	10.597261	-0.056983	4.816196
277.240875	8000.153730	10.602266	-0.056981	4.816113
277.146724	8000.123184	10.607271	-0.056964	4.816104
277.192707	8000.130436	10.612275	-0.056973	4.816106
277.215475	7999.958849	10.617280	-0.056977	4.816056
277.150142	8000.242927	10.622285	-0.056965	4.816139
277.243731	8000.189076	10.627290	-0.056982	4.816123
277.187465	8000.240413	10.632295	-0.056972	4.816138
277.121334	8000.370633	10.637299	-0.056960	4.816177
277.275735	7999.910834	10.642304	-0.056988	4.816041
277.148339	8000.329470	10.647309	-0.056965	4.816164
277.362055	8000.273525	10.652314	-0.057005	4.816147
277.291720	8000.279735	10.657319	-0.056992	4.816149
277.256467	8000.278035	10.662323	-0.056985	4.816149
277.295668	8000.104608	10.667328	-0.056993	4.816098
277.141427	8000.288784	10.672333	-0.056964	4.816153
277.384625	8000.192775	10.677338	-0.057009	4.816123
277.279438	8000.209037	10.682343	-0.056990	4.816128
277.259293	8000.292013	10.687347	-0.056986	4.816153
277.512847	8000.194055	10.692352	-0.057034	4.816123
277.333071	8000.368154	10.697357	-0.057000	4.816175
277.171456	8000.144075	10.702362	-0.056970	4.816110
277.287612	8000.251958	10.707367	-0.056992	4.816141
277.249556	8000.272643	10.712371	-0.056985	4.816147
277.353736	8000.052318	10.717376	-0.057004	4.816082
277.390682	8000.380989	10.722381	-0.057011	4.816178
277.445953	8000.376657	10.727386	-0.057022	4.816177
277.496868	8000.336989	10.732391	-0.057031	4.816165
277.300745	8000.473398	10.737395	-0.056995	4.816206
277.263681	8000.412903	10.742400	-0.056988	4.816188
277.196393	8000.648875	10.747405	-0.056976	4.816257
277.288425	8000.396273	10.752410	-0.056993	4.816183
277.516347	8000.173917	10.757415	-0.057035	4.816117
277.320094	8000.400068	10.762419	-0.056999	4.816184
277.475757	8000.163580	10.767424	-0.057028	4.816114
277.377700	8000.373350	10.772429	-0.057010	4.816176
277.345059	8000.254174	10.777434	-0.057004	4.816141
277.277958	8000.429249	10.782439	-0.056991	4.816193
277.273801	8000.450549	10.787443	-0.056991	4.816199
277.327971	8000.289143	10.792448	-0.057001	4.816152
277.257488	8000.487662	10.797453	-0.056988	4.816210
277.440981	8000.399116	10.802458	-0.057022	4.816183
277.433387	8000.391507	10.807463	-0.057021	4.816181
277.302572	8000.401962	10.812467	-0.056996	4.816185
277.288815	8000.172017	10.817472	-0.056994	4.816118
277.304070	8000.403073	10.822477	-0.056997	4.816185
277.546654	8000.220513	10.827482	-0.057042	4.816130
277.480950	8000.520616	10.832487	-0.057030	4.816218
277.570887	8000.380158	10.837491	-0.057047	4.816177
277.573131	8000.129134	10.842496	-0.057047	4.816104
277.392345	8000.382276	10.847501	-0.057014	4.816178
277.504556	8000.217650	10.852506	-0.057034	4.816130
277.620462	8000.412071	10.857511	-0.057056	4.816186
277.315297	8000.400132	10.862515	-0.057000	4.816184
277.395713	8000.143048	10.867520	-0.057014	4.816109
277.522229	8000.397490	10.872525	-0.057038	4.816182
277.485104	8000.271822	10.877530	-0.057031	4.816146
277.444076	8000.265744	10.882535	-0.057024	4.816144
277.372081	8000.402268	10.887539	-0.057010	4.816184
277.499336	8000.131076	10.892544	-0.057034	4.816104
277.287215	8000.324887	10.897549	-0.056995	4.816162
277.332468	8000.405845	10.902554	-0.057003	4.816186
277.411556	8000.400877	10.907559	-0.057018	4.816184
277.353010	8000.467132	10.912563	-0.057007	4.816203
277.356049	8000.311209	10.917568	-0.057008	4.816158
277.566651	8000.299011	10.922573	-0.057047	4.816153
277.603222	8000.368059	10.927578	-0.057054	4.816173
277.465226	8000.327101	10.932583	-0.057028	4.816162
277.461296	8000.350542	10.937587	-0.057028	4.816169
277.641675	8000.223478	10.942592	-0.057061	4.816131
277.552121	8000.474002	10.947597	-0.057045	4.816204
277.444972	8000.414372	10.952602	-0.057025	4.816187
277.533932	8000.298470	10.957607	-0.057042	4.816153
277.569744	8000.502123	10.962611	-0.057049	4.816212
277.620628	8000.284032	10.967616	-0.057058	4.816148
277.532383	8000.377526	10.972621	-0.057042	4.816176
277.489371	8000.085083	10.977626	-0.057034	4.816091
277.379952	8000.270073	10.982631	-0.057013	4.816146
277.348793	8000.318661	10.987635	-0.057008	4.816160
277.507620	8000.091847	10.992640	-0.057037	4.816093
277.567843	8000.326924	10.997645	-0.057049	4.816161
277.616400	8000.302171	11.002650	-0.057058	4.816154
277.761717	8000.237506	11.007655	-0.057085	4.816134
277.686915	8000.427400	11.012659	-0.057071	4.816190
277.448794	8000.272443	11.017664	-0.057027	4.816146
277.500110	8000.357785	11.022669	-0.057036	4.816171
277.582528	8000.351809	11.027674	-0.057052	4.816168
277.640169	8000.396666	11.032679	-0.057063	4.816181
277.454083	8000.472359	11.037683	-0.057028	4.816204
277.550224	8000.258295	11.042688	-0.057046	4.816141
277.332534	8000.374013	11.047693	-0.057006	4.816176
277.441070	8000.241372	11.052698	-0.057026	4.816137
277.356710	8000.489854	11.057703	-0.057010	4.816210
277.219230	8000.525829	11.062707	-0.056985	4.816221
277.346696	8000.419173	11.067712	-0.057009	4.816189
277.500889	8000.236077	11.072717	-0.057037	4.816135
277.764251	8000.224836	11.077722	-0.057086	4.816130
277.689628	8000.273705	11.082727	-0.057073	4.816145
277.509711	8000.518317	11.087731	-0.057039	4.816217
277.774872	8000.195137	11.092736	-0.057089	4.816122
277.687713	8000.367712	11.097741	-0.057072	4.816173
277.669091	8000.449648	11.102746	-0.057069	4.816197
277.798375	8000.354777	11.107751	-0.057093	4.816168
277.803162	8000.574964	11.112755	-0.057094	4.816232
277.689502	8000.317559	11.117760	-0.057073	4.816158
277.413947	8000.438639	11.122765	-0.057022	4.816195
277.537079	8000.282757	11.127770	-0.057045	4.816148
277.690120	8000.286610	11.132775	-0.057073	4.816149
277.520800	8000.444874	11.137779	-0.057042	4.816196
277.647965	8000.124533	11.142784	-0.057066	4.816102
277.655193	8000.403523	11.147789	-0.057067	4.816183
277.731391	8000.430554	11.152794	-0.057082	4.816191
277.678414	8000.372975	11.157799	-0.057072	4.816174
277.620134	8000.468082	11.162803	-0.057061	4.816202
277.660878	8000.512633	11.167808	-0.057069	4.816215
277.866282	8000.316576	11.172813	-0.057107	4.816157
277.938633	8000.320033	11.177818	-0.057120	4.816157
277.596565	8000.312766	11.182823	-0.057057	4.816157
277.481367	8000.486970	11.187827	-0.057036	4.816208
277.626949	8000.324016	11.192832	-0.057063	4.816160
277.737223	8000.421112	11.197837	-0.057083	4.816188
277.751402	8000.352999	11.202842	-0.057086	4.816168
277.819350	8000.664080	11.207847	-0.057099	4.816258
277.591652	8000.585165	11.212851	-0.057057	4.816237
277.689915	8000.176690	11.217856	-0.057075	4.816117
277.554044	8000.314192	11.222861	-0.057049	4.816158
277.516849	8000.306046	11.227866	-0.057043	4.816155
277.623500	8000.487480	11.232871	-0.057063	4.816208
277.520506	8000.386257	11.237875	-0.057044	4.816179
277.852014	8000.463863	11.242880	-0.057105	4.816200
277.792764	8000.536516	11.247885	-0.057094	4.816221
277.894950	8000.317217	11.252890	-0.057113	4.816157
277.896109	8000.196516	11.257895	-0.057114	4.816121
277.644356	8000.358626	11.262899	-0.057067	4.816170
277.730697	8000.324943	11.267904	-0.057083	4.816160
277.597659	8000.386641	11.272909	-0.057058	4.816178
277.728089	8000.413588	11.277914	-0.057083	4.816186
277.898184	8000.328005	11.282919	-0.057115	4.816160
277.458518	8000.502732	11.287923	-0.057033	4.816213
277.627022	8000.370110	11.292928	-0.057064	4.816173
277.640788	8000.644948	11.297933	-0.057067	4.816254
277.756588	8000.472906	11.302938	-0.057089	4.816203
277.783668	8000.573836	11.307943	-0.057094	4.816232
277.728950	8000.534387	11.312947	-0.057084	4.816221
277.815672	8000.451564	11.317952	-0.057100	4.816196
277.690774	8000.448237	11.322957	-0.057077	4.816196
277.709048	8000.393019	11.327962	-0.057080	4.816180
277.850559	8000.315463	11.332967	-0.057106	4.816156
277.937293	8000.386491	11.337971	-0.057123	4.816177
277.852726	8000.267440	11.342976	-0.057107	4.816142
277.876678	8000.536052	11.347981	-0.057112	4.816221
277.912140	8000.405289	11.352986	-0.057118	4.816182
277.793294	8000.439466	11.357991	-0.057096	4.816193
277.864654	8000.576457	11.362995	-0.057110	4.816232
277.791542	8000.418081	11.368000	-0.057096	4.816187
277.752823	8000.216526	11.373005	-0.057089	4.816128
277.750248	8000.062639	11.378010	-0.057088	4.816083
277.768541	8000.211485	11.383015	-0.057092	4.816126
277.682355	8000.525107	11.388019	-0.057076	4.816218
277.698470	8000.458097	11.393024	-0.057079	4.816199
277.788250	8000.422340	11.398029	-0.057096	4.816188
277.707560	8000.258486	11.403034	-0.057081	4.816140
277.793627	8000.347664	11.408039	-0.057097	4.816166
277.671671	8000.454436	11.413043	-0.057074	4.816198
277.846534	8000.398854	11.418048	-0.057107	4.816181
277.727485	8000.386017	11.423053	-0.057085	4.816178
277.934322	8000.281869	11.428058	-0.057123	4.816146
277.916322	8000.530490	11.433063	-0.057120	4.816219
277.863210	8000.459018	11.438067	-0.057110	4.816198
277.749711	8000.245422	11.443072	-0.057089	4.816136
277.669478	8000.407439	11.448077	-0.057075	4.816184
277.627466	8000.405616	11.453082	-0.057067	4.816184
277.885043	8000.295978	11.458087	-0.057115	4.816150
277.899984	8000.571907	11.463091	-0.057118	4.816231
277.791851	8000.337038	11.468096	-0.057098	4.816163
277.597842	8000.535454	11.473101	-0.057062	4.816222
277.845521	8000.447005	11.478106	-0.057108	4.816195
277.925218	8000.245461	11.483111	-0.057123	4.816135
277.873217	8000.193242	11.488115	-0.057113	4.816120
277.899538	8000.294157	11.493120	-0.057118	4.816150
277.972103	8000.371338	11.498125	-0.057132	4.816172
277.997364	8000.363256	11.503130	-0.057136	4.816169
277.991297	8000.106738	11.508135	-0.057135	4.816094
277.725945	8000.449161	11.513139	-0.057086	4.816196
277.940843	8000.362253	11.518144	-0.057126	4.816169
277.740745	8000.294526	11.523149	-0.057089	4.816151
277.887570	8000.135870	11.528154	-0.057116	4.816104
277.833422	8000.367806	11.533159	-0.057106	4.816172
277.704034	8000.562053	11.538163	-0.057082	4.816229
277.841105	8000.151075	11.543168	-0.057108	4.816108
277.804920	8000.407911	11.548173	-0.057101	4.816183
277.958182	8000.386126	11.553178	-0.057130	4.816176
277.919527	8000.390774	11.558183	-0.057123	4.816178
277.793930	8000.512438	11.563187	-0.057100	4.816214
278.062258	8000.317522	11.568192	-0.057149	4.816156
277.691011	8000.570417	11.573197	-0.057081	4.816232
277.629220	8000.396221	11.578202	-0.057069	4.816181
278.036772	8000.192079	11.583207	-0.057145	4.816119
278.016160	8000.408599	11.588211	-0.057141	4.816182
278.042150	8000.177234	11.593216	-0.057146	4.816115
277.968511	8000.139580	11.598221	-0.057132	4.816104
277.944654	8000.332535	11.603226	-0.057128	4.816161
277.875835	7999.980861	11.608231	-0.057115	4.816058
277.802193	8000.243425	11.613235	-0.057102	4.816135
277.918105	8000.009421	11.618240	-0.057123	4.816066
277.662022	8000.323164	11.623245	-0.057076	4.816159
277.682819	8000.355601	11.628250	-0.057080	4.816169
277.789790	8000.078698	11.633255	-0.057100	4.816087
277.902318	8000.497424	11.638259	-0.057121	4.816209
277.832799	8000.480143	11.643264	-0.057108	4.816204
277.840591	8000.433282	11.648269	-0.057110	4.816191
278.061893	8000.485384	11.653274	-0.057151	4.816205
277.918960	8000.215696	11.658279	-0.057124	4.816127
277.793800	8000.563870	11.663283	-0.057101	4.816229
277.939895	8000.306905	11.668288	-0.057128	4.816153
277.909324	8000.509356	11.673293	-0.057123	4.816212
277.780552	8000.362791	11.678298	-0.057099	4.816170
278.006745	8000.275020	11.683303	-0.057141	4.816143
277.811214	8000.452041	11.688307	-0.057105	4.816196
277.971530	8000.345980	11.693312	-0.057135	4.816164
277.885597	8000.429901	11.698317	-0.057119	4.816189
278.003883	8000.386113	11.703322	-0.057141	4.816176
277.857391	8000.377052	11.708327	-0.057114	4.816174
277.716240	8000.481339	11.713331	-0.057087	4.816205
277.792259	8000.297892	11.718336	-0.057101	4.816151
277.779299	8000.378863	11.723341	-0.057099	4.816175
277.589729	8000.349789	11.728346	-0.057064	4.816168
277.854850	8000.285161	11.733351	-0.057113	4.816147
277.952512	8000.460022	11.738355	-0.057132	4.816198
277.913463	8000.158031	11.743360	-0.057124	4.816110
277.706761	8000.360490	11.748365	-0.057086	4.816170
277.931173	8000.272686	11.753370	-0.057128	4.816143
277.991986	8000.159478	11.758375	-0.057139	4.816110
277.880479	8000.349775	11.763379	-0.057119	4.816166
277.837411	8000.185536	11.768384	-0.057111	4.816118
277.982186	8000.425356	11.773389	-0.057138	4.816187
277.879573	8000.207684	11.778394	-0.057119	4.816124
277.862070	8000.246904	11.783399	-0.057115	4.816136
277.932360	8000.270624	11.788403	-0.057129	4.816143
277.975449	8000.288507	11.793408	-0.057137	4.816148
278.028562	8000.407004	11.798413	-0.057147	4.816182
278.055814	8000.436353	11.803418	-0.057152	4.816190
278.021538	8000.440012	11.808423	-0.057146	4.816192
277.948932	8000.466481	11.813427	-0.057132	4.816200
277.892170	8000.210109	11.818432	-0.057122	4.816125
277.873743	8000.296323	11.823437	-0.057118	4.816150
277.801485	8000.178564	11.828442	-0.057105	4.816116
277.895457	8000.247586	11.833447	-0.057122	4.816136
277.782418	8000.171823	11.838451	-0.057101	4.816114
278.081554	8000.216788	11.843456	-0.057157	4.816126
277.928139	8000.292006	11.848461	-0.057129	4.816149
277.886767	8000.309425	11.853466	-0.057121	4.816154
277.996101	8000.375521	11.858471	-0.057142	4.816173
277.998617	8000.623448	11.863475	-0.057142	4.816245
278.000648	8000.208947	11.868480	-0.057143	4.816124
277.990574	8000.505790	11.873485	-0.057141	4.816211
278.044775	8000.305920	11.878490	-0.057151	4.816152
278.030625	8000.262934	11.883495	-0.057148	4.816140
278.139786	8000.198681	11.888499	-0.057169	4.816120
278.238959	8000.158820	11.893504	-0.057187	4.816108
278.036496	8000.093188	11.898509	-0.057150	4.816090
277.936036	8000.263385	11.903514	-0.057131	4.816140
278.291496	8000.436515	11.908519	-0.057197	4.816189
278.117647	8000.346826	11.913523	-0.057165	4.816164
278.125094	8000.173887	11.918528	-0.057166	4.816113
278.045090	8000.412834	11.923533	-0.057152	4.816183
278.256554	8000.446595	11.928538	-0.057191	4.816192
278.198767	8000.393201	11.933543	-0.057181	4.816177
277.960906	8000.463681	11.938547	-0.057136	4.816199
278.218747	8000.136092	11.943552	-0.057184	4.816102
278.258375	8000.140024	11.948557	-0.057192	4.816103
278.105684	8000.435347	11.953562	-0.057164	4.816190
278.051030	8000.392695	11.958567	-0.057153	4.816178
278.055671	8000.467576	11.963571	-0.057154	4.816199
278.011911	8000.299048	11.968576	-0.057146	4.816150
278.130799	8000.479639	11.973581	-0.057169	4.816202
278.201732	8000.319602	11.978586	-0.057182	4.816155
278.188577	8000.328987	11.983591	-0.057179	4.816158
278.093178	8000.625353	11.988595	-0.057162	4.816245
278.098611	8000.526095	11.993600	-0.057163	4.816216
278.214531	8000.349780	11.998605	-0.057184	4.816164
278.096927	8000.298507	12.003610	-0.057163	4.816150
278.276699	8000.015444	12.008615	-0.057196	4.816066
278.328678	8000.562354	12.013619	-0.057206	4.816226
278.161603	8000.176836	12.018624	-0.057175	4.816114
278.180330	8000.254109	12.023629	-0.057178	4.816136
278.120306	8000.413289	12.028634	-0.057167	4.816183
278.089465	8000.236449	12.033639	-0.057162	4.816132
278.089054	8000.556974	12.038643	-0.057162	4.816225
278.235777	8000.247666	12.043648	-0.057189	4.816134
278.121691	8000.194320	12.048653	-0.057168	4.816119
278.081041	8000.200001	12.053658	-0.057160	4.816121
278.282995	8000.285940	12.058663	-0.057198	4.816145
278.002212	8000.418678	12.063667	-0.057146	4.816185
278.127825	8000.451949	12.068672	-0.057169	4.816194
278.072491	8000.469115	12.073677	-0.057159	4.816200
278.192048	8000.376203	12.078682	-0.057182	4.816172
278.177026	8000.290465	12.083687	-0.057179	4.816147
278.068632	8000.437015	12.088691	-0.057159	4.816190
278.405016	8000.364065	12.093696	-0.057221	4.816167
278.346437	8000.327751	12.098701	-0.057211	4.816157
278.172423	8000.232718	12.103706	-0.057178	4.816130
278.270799	8000.151175	12.108711	-0.057197	4.816106
278.264827	8000.428861	12.113715	-0.057196	4.816187
278.255224	8000.179754	12.118720	-0.057194	4.816114
278.322157	8000.428848	12.123725	-0.057207	4.816187
278.295717	8000.364271	12.128730	-0.057202	4.816168
278.342484	7999.900371	12.133735	-0.057210	4.816032
278.020476	8000.254587	12.138739	-0.057150	4.816137
278.333429	8000.191895	12.143744	-0.057209	4.816117
278.104927	8000.477296	12.148749	-0.057166	4.816202
278.250573	8000.430800	12.153754	-0.057194	4.816187
278.236490	8000.204048	12.158759	-0.057191	4.816121
278.222250	8000.291407	12.163763	-0.057188	4.816147
278.180452	8000.393223	12.168768	-0.057181	4.816177
278.264259	8000.290047	12.173773	-0.057196	4.816146
278.394692	8000.338363	12.178778	-0.057221	4.816160
278.469693	8000.131391	12.183783	-0.057235	4.816099
278.397758	8000.407882	12.188787	-0.057222	4.816180
278.283581	8000.110935	12.193792	-0.057200	4.816094
278.317049	8000.355148	12.198797	-0.057207	4.816165
278.078674	8000.175611	12.203802	-0.057162	4.816114
278.329395	8000.063711	12.208807	-0.057209	4.816080
278.265049	8000.379869	12.213811	-0.057197	4.816173
278.201245	8000.054991	12.218816	-0.057185	4.816078
278.244414	8000.274805	12.223821	-0.057193	4.816142
278.319419	8000.276173	12.228826	-0.057208	4.816142
278.367916	8000.141373	12.233831	-0.057217	4.816102
278.155249	8000.491166	12.238835	-0.057177	4.816206
278.387721	8000.166320	12.243840	-0.057220	4.816109
278.423917	8000.207584	12.248845	-0.057227	4.816121
278.178769	8000.376226	12.253850	-0.057182	4.816172
278.246240	8000.194760	12.258855	-0.057194	4.816118
278.262524	8000.281604	12.263859	-0.057197	4.816144
278.399311	8000.123832	12.268864	-0.057223	4.816097
278.412541	8000.379431	12.273869	-0.057226	4.816172
278.451137	8000.423944	12.278874	-0.057233	4.816184
278.260552	8000.175826	12.283879	-0.057197	4.816113
278.162083	8000.443287	12.288883	-0.057179	4.816192
278.357559	8000.471416	12.293888	-0.057216	4.816199
278.289190	8000.537493	12.298893	-0.057203	4.816218
278.139779	8000.419399	12.303898	-0.057175	4.816185
278.497467	8000.105374	12.308903	-0.057242	4.816091
278.516143	8000.496762	12.313907	-0.057246	4.816205
278.533900	8000.402001	12.318912	-0.057249	4.816178
278.575373	8000.462594	12.323917	-0.057257	4.816195
278.748634	8000.430488	12.328922	-0.057289	4.816185
278.489276	8000.295440	12.333927	-0.057241	4.816147
278.263981	8000.413159	12.338931	-0.057199	4.816182
278.391902	7999.974235	12.343936	-0.057223	4.816053
278.515308	8000.166657	12.348941	-0.057246	4.816109
278.375859	8000.069046	12.353946	-0.057220	4.816081
278.370440	8000.181138	12.358951	-0.057219	4.816114
278.294627	8000.165881	12.363955	-0.057205	4.816110
278.367458	8000.099900	12.368960	-0.057219	4.816090
278.253607	8000.166220	12.373965	-0.057197	4.816110
278.247309	8000.230217	12.378970	-0.057196	4.816129
278.268532	8000.260526	12.383975	-0.057200	4.816138
278.179127	8000.430926	12.388979	-0.057184	4.816188
278.489247	8000.384209	12.393984	-0.057242	4.816173
278.422708	8000.376598	12.398989	-0.057229	4.816171
278.324429	8000.425038	12.403994	-0.057211	4.816185
278.380138	8000.377978	12.408999	-0.057222	4.816171
278.489842	8000.270997	12.414003	-0.057242	4.816139
278.560495	8000.280834	12.419008	-0.057255	4.816142
278.302985	8000.306084	12.424013	-0.057208	4.816151
278.370296	8000.252824	12.429018	-0.057220	4.816135
278.414111	8000.153196	12.434023	-0.057228	4.816105
278.311159	8000.384250	12.439027	-0.057209	4.816173
278.314777	8000.047774	12.444032	-0.057210	4.816075
278.415923	8000.103037	12.449037	-0.057229	4.816091
278.379109	8000.142976	12.454042	-0.057222	4.816103
278.340144	8000.236296	12.459047	-0.057215	4.816130
278.258344	8000.457050	12.464051	-0.057200	4.816195
278.254978	8000.049932	12.469056	-0.057199	4.816076
278.404517	8000.171245	12.474061	-0.057227	4.816111
278.374507	8000.265797	12.479066	-0.057222	4.816138
278.544007	8000.222939	12.484071	-0.057253	4.816125
278.571982	8000.509792	12.489075	-0.057259	4.816209
278.461367	8000.182991	12.494080	-0.057238	4.816114
278.624809	8000.194512	12.499085	-0.057269	4.816116
278.426313	8000.170618	12.504090	-0.057232	4.816110
278.425272	8000.124665	12.509095	-0.057231	4.816097
278.397763	8000.350677	12.514099	-0.057227	4.816163
278.601969	8000.272122	12.519104	-0.057265	4.816139
278.468771	8000.230181	12.524109	-0.057240	4.816128
278.515502	8000.270568	12.529114	-0.057249	4.816139
278.721381	8000.036055	12.534119	-0.057287	4.816069
278.509477	8000.310005	12.539123	-0.057248	4.816151
278.409574	8000.178922	12.544128	-0.057229	4.816113
278.429415	7999.990182	12.549133	-0.057233	4.816058
278.451197	8000.175418	12.554138	-0.057237	4.816112
278.506748	8000.090961	12.559143	-0.057247	4.816087
278.640173	8000.400026	12.564147	-0.057273	4.816176
278.502680	7999.990472	12.569152	-0.057247	4.816057
278.532044	8000.165163	12.574157	-0.057252	4.816108
278.648761	8000.254899	12.579162	-0.057274	4.816134
278.555411	7999.965810	12.584167	-0.057257	4.816050
278.569816	8000.229976	12.589171	-0.057260	4.816127
278.355725	8000.088274	12.594176	-0.057220	4.816087
278.403149	8000.088073	12.599181	-0.057229	4.816086
278.188831	8000.273300	12.604186	-0.057189	4.816142
278.478853	7999.965527	12.609191	-0.057243	4.816050
278.541942	8000.055357	12.614195	-0.057255	4.816076
278.410350	8000.243153	12.619200	-0.057230	4.816132
278.323976	8000.236252	12.624205	-0.057214	4.816130
278.460191	8000.182105	12.629210	-0.057240	4.816114
278.662437	8000.177235	12.634215	-0.057278	4.816111
278.365839	8000.374860	12.639219	-0.057223	4.816170
278.320736	8000.387938	12.644224	-0.057214	4.816174
278.541364	8000.250918	12.649229	-0.057255	4.816133
278.455910	8000.272880	12.654234	-0.057240	4.816140
278.521443	8000.113815	12.659239	-0.057252	4.816093
278.548927	8000.286336	12.664243	-0.057257	4.816143
278.467601	7999.989987	12.669248	-0.057242	4.816057
278.495969	8000.194575	12.674253	-0.057247	4.816117
278.389644	8000.221500	12.679258	-0.057228	4.816125
278.403932	8000.167278	12.684263	-0.057230	4.816109
278.368862	8000.098271	12.689267	-0.057224	4.816089
278.395246	8000.068842	12.694272	-0.057229	4.816081
278.455300	8000.090239	12.699277	-0.057240	4.816087
278.511549	8000.173534	12.704282	-0.057251	4.816111
278.351372	8000.331966	12.709287	-0.057221	4.816158
278.252917	8000.333392	12.714291	-0.057203	4.816159
278.494184	8000.235210	12.719296	-0.057248	4.816129
278.520209	8000.166243	12.724301	-0.057252	4.816109
278.501590	8000.037703	12.729306	-0.057249	4.816071
278.498600	7999.957527	12.734311	-0.057248	4.816048
278.588957	8000.445303	12.739315	-0.057266	4.816190
278.439658	8000.040876	12.744320	-0.057238	4.816072
278.396448	8000.066810	12.749325	-0.057230	4.816080
278.480548	8000.276683	12.754330	-0.057246	4.816141
278.589358	8000.253023	12.759335	-0.057266	4.816133
278.519080	8000.265645	12.764339	-0.057253	4.816138
278.514147	8000.051881	12.769344	-0.057252	4.816075
278.526160	8000.123689	12.774349	-0.057254	4.816096
278.361679	8000.112165	12.779354	-0.057224	4.816094
278.479092	8000.107893	12.784359	-0.057246	4.816092
278.483202	8000.282126	12.789363	-0.057247	4.816143
278.462513	8000.093718	12.794368	-0.057243	4.816088
278.497303	8000.319792	12.799373	-0.057249	4.816153
278.586634	8000.292573	12.804378	-0.057266	4.816145
278.637167	8000.107593	12.809383	-0.057276	4.816091
278.460120	8000.385382	12.814387	-0.057243	4.816173
278.565987	8000.087086	12.819392	-0.057262	4.816085
278.581073	8000.194208	12.824397	-0.057265	4.816116
278.560258	8000.386154	12.829402	-0.057262	4.816173
278.809997	7999.873581	12.834407	-0.057308	4.816021
278.814130	8000.108713	12.839411	-0.057309	4.816090
278.560183	7999.962015	12.844416	-0.057262	4.816049
278.617198	8000.013272	12.849421	-0.057272	4.816063
278.529904	8000.291619	12.854426	-0.057256	4.816145
278.609691	7999.952251	12.859431	-0.057271	4.816045
278.415761	8000.173106	12.864435	-0.057235	4.816111
278.593078	7999.887861	12.869440	-0.057268	4.816027
278.509964	8000.027390	12.874445	-0.057253	4.816068
278.566265	8000.050855	12.879450	-0.057263	4.816074
278.756767	7999.913290	12.884455	-0.057299	4.816033
278.702297	8000.147359	12.889459	-0.057289	4.816102
278.836831	7999.967109	12.894464	-0.057314	4.816049
278.590343	8000.032091	12.899469	-0.057268	4.816069
278.470240	8000.088682	12.904474	-0.057246	4.816086
278.834197	7999.967084	12.909479	-0.057314	4.816049
278.521627	8000.364212	12.914483	-0.057256	4.816166
278.651521	8000.319567	12.919488	-0.057280	4.816153
278.775738	8000.100665	12.924493	-0.057303	4.816088
278.697680	8000.195414	12.929498	-0.057289	4.816116
278.645765	7999.984003	12.934503	-0.057279	4.816054
278.555379	7999.925745	12.939507	-0.057262	4.816038
278.528344	7999.986161	12.944512	-0.057257	4.816056
278.312349	8000.111527	12.949517	-0.057217	4.816094
278.383459	8000.387407	12.954522	-0.057231	4.816174
278.605883	8000.089089	12.959527	-0.057272	4.816085
278.448011	8000.299915	12.964531	-0.057243	4.816148
278.563752	8000.331939	12.969536	-0.057265	4.816157
278.672745	8000.068956	12.974541	-0.057285	4.816079
278.606700	8000.256875	12.979546	-0.057273	4.816134
278.519011	7999.936906	12.984551	-0.057256	4.816041
278.626849	8000.295719	12.989555	-0.057277	4.816146
278.799744	8000.398229	12.994560	-0.057309	4.816175
278.661058	8000.269644	12.999565	-0.057283	4.816138
278.556699	8000.446185	13.004570	-0.057264	4.816190
278.613728	8000.134180	13.009575	-0.057274	4.816099
278.560101	8000.464425	13.014579	-0.057265	4.816195
278.567562	8000.040406	13.019584	-0.057266	4.816071
278.688543	8000.259497	13.024589	-0.057289	4.816135
278.600062	8000.397862	13.029594	-0.057272	4.816176
278.563266	8000.155739	13.034599	-0.057265	4.816105
278.678210	8000.362969	13.039603	-0.057287	4.816165
278.734406	8000.251812	13.044608	-0.057297	4.816132
278.688034	8000.395215	13.049613	-0.057289	4.816174
278.520103	8000.433843	13.054618	-0.057258	4.816187
278.681096	8000.261551	13.059623	-0.057288	4.816135
278.517959	8000.532115	13.064627	-0.057258	4.816215
278.711578	8000.230067	13.069632	-0.057294	4.816126
278.665296	8000.377745	13.074637	-0.057285	4.816169
278.449443	8000.455036	13.079642	-0.057245	4.816193
278.608636	8000.265616	13.084647	-0.057275	4.816137
278.544653	8000.313610	13.089651	-0.057263	4.816151
278.577496	8000.377250	13.094656	-0.057269	4.816170
278.696952	8000.081337	13.099661	-0.057291	4.816083
278.774747	8000.520811	13.104666	-0.057306	4.816211
278.823688	8000.086857	13.109671	-0.057315	4.816084
278.544848	8000.285872	13.114675	-0.057263	4.816143
278.499483	8000.448525	13.119680	-0.057255	4.816191
278.649800	8000.385019	13.124685	-0.057283	4.816172
278.781240	8000.519898	13.129690	-0.057308	4.816210
278.715366	8000.292202	13.134695	-0.057295	4.816144
278.787322	8000.543530	13.139699	-0.057309	4.816217
278.766947	8000.280332	13.144704	-0.057305	4.816140
278.853441	8000.113099	13.149709	-0.057321	4.816091
278.781737	8000.241084	13.154714	-0.057308	4.816129
278.749990	8000.031106	13.159719	-0.057302	4.816068
278.695880	8000.454295	13.164723	-0.057292	4.816192
278.740657	8000.087577	13.169728	-0.057300	4.816084
278.906314	8000.304276	13.174733	-0.057331	4.816147
278.728335	8000.436743	13.179738	-0.057298	4.816186
278.741182	8000.419889	13.184743	-0.057301	4.816181
278.706625	8000.369053	13.189747	-0.057295	4.816167
278.828065	8000.187495	13.194752	-0.057317	4.816113
278.801951	8000.209466	13.199757	-0.057312	4.816119
278.638319	8000.389205	13.204762	-0.057282	4.816173
278.697258	8000.197965	13.209767	-0.057293	4.816117
278.587951	8000.343431	13.214771	-0.057273	4.816160
278.694245	8000.244936	13.219776	-0.057293	4.816130
278.864037	8000.156141	13.224781	-0.057324	4.816104
278.831513	8000.542331	13.229786	-0.057319	4.816217
278.884834	8000.204612	13.234791	-0.057328	4.816118
278.930697	8000.380675	13.239795	-0.057337	4.816169
278.962215	8000.269069	13.244800	-0.057343	4.816136
278.910387	8000.399553	13.249805	-0.057333	4.816174
278.631779	8000.532331	13.254810	-0.057282	4.816215
278.863316	8000.571802	13.259815	-0.057325	4.816225
278.792888	8000.372869	13.264819	-0.057312	4.816167
278.789325	8000.299090	13.269824	-0.057311	4.816146
278.969436	8000.548108	13.274829	-0.057345	4.816217
278.720747	8000.545737	13.279834	-0.057299	4.816218
278.762736	8000.428979	13.284839	-0.057306	4.816184
278.700489	8000.429993	13.289843	-0.057295	4.816184
278.743421	7999.999138	13.294848	-0.057303	4.816058
278.824523	8000.458971	13.299853	-0.057318	4.816192
278.809475	8000.530291	13.304858	-0.057316	4.816213
279.149684	8000.375140	13.309863	-0.057379	4.816166
279.035590	8000.578218	13.314867	-0.057358	4.816226
278.773227	8000.388622	13.319872	-0.057309	4.816172
278.827064	8000.135321	13.324877	-0.057319	4.816098
278.790756	8000.330191	13.329882	-0.057312	4.816155
278.749260	8000.337993	13.334887	-0.057305	4.816157
278.735211	8000.296077	13.339891	-0.057302	4.816145
278.764645	8000.330808	13.344896	-0.057308	4.816155
278.819374	8000.301893	13.349901	-0.057318	4.816146
278.663160	8000.390950	13.354906	-0.057289	4.816173
278.724673	8000.197620	13.359911	-0.057300	4.816116
278.698634	8000.235619	13.364915	-0.057296	4.816128
278.927279	8000.457737	13.369920	-0.057338	4.816191
278.856517	8000.084646	13.374925	-0.057325	4.816083
278.876914	8000.358541	13.379930	-0.057329	4.816163
278.879646	8000.267782	13.384935	-0.057330	4.816136
278.735557	8000.410480	13.389939	-0.057303	4.816178
278.916677	8000.258853	13.394944	-0.057337	4.816133
278.970466	8000.355996	13.399949	-0.057347	4.816161
278.786136	8000.491554	13.404954	-0.057313	4.816202
278.895502	8000.181565	13.409959	-0.057333	4.816111
278.843263	8000.444526	13.414963	-0.057324	4.816188
278.890551	8000.265895	13.419968	-0.057332	4.816135
278.919323	8000.242920	13.424973	-0.057338	4.816128
278.842197	8000.468035	13.429978	-0.057324	4.816195
278.975268	8000.309125	13.434983	-0.057348	4.816148
278.620760	8000.218292	13.439987	-0.057282	4.816123
278.884182	8000.272228	13.444992	-0.057331	4.816137
278.812938	8000.171579	13.449997	-0.057318	4.816108
278.608740	8000.272586	13.455002	-0.057280	4.816139
278.845332	7999.998030	13.460007	-0.057324	4.816057
278.998572	8000.304251	13.465011	-0.057353	4.816146
278.901824	8000.274723	13.470016	-0.057335	4.816138
278.833567	8000.368582	13.475021	-0.057323	4.816166
278.941838	8000.341707	13.480026	-0.057343	4.816157
278.894912	8000.082304	13.485031	-0.057334	4.816082
278.826180	8000.409071	13.490035	-0.057321	4.816178
278.895493	8000.262893	13.495040	-0.057334	4.816134
278.944930	8000.301193	13.500045	-0.057344	4.816145
278.778042	8000.273597	13.505050	-0.057313	4.816138
278.841547	8000.304674	13.510055	-0.057325	4.816147
278.918191	8000.339194	13.515059	-0.057339	4.816157
278.726484	8000.359227	13.520064	-0.057303	4.816163
278.732153	8000.170226	13.525069	-0.057304	4.816108
278.717686	8000.412504	13.530074	-0.057302	4.816179
278.925297	8000.214346	13.535079	-0.057340	4.816120
278.853021	8000.401086	13.540083	-0.057327	4.816175
278.904266	8000.387066	13.545088	-0.057337	4.816171
278.892669	8000.550335	13.550093	-0.057335	4.816218
278.814988	8000.567095	13.555098	-0.057320	4.816224
279.008618	8000.000075	13.560103	-0.057356	4.816057
278.941121	8000.176216	13.565107	-0.057344	4.816109
279.079877	8000.294132	13.570112	-0.057370	4.816143
279.078845	8000.350748	13.575117	-0.057370	4.816159
278.928401	8000.437773	13.580122	-0.057342	4.816185
279.100041	8000.180198	13.585127	-0.057374	4.816109
278.872112	8000.361976	13.590131	-0.057332	4.816163
278.833464	8000.184991	13.595136	-0.057324	4.816112
279.149658	8000.109537	13.600141	-0.057383	4.816088
278.836612	8000.417981	13.605146	-0.057325	4.816180
279.040108	8000.258212	13.610151	-0.057363	4.816132
279.121426	8000.274654	13.615155	-0.057378	4.816137
279.104513	8000.062806	13.620160	-0.057375	4.816075
279.153681	8000.028448	13.625165	-0.057384	4.816064
279.095719	8000.182325	13.630170	-0.057374	4.816110
279.280556	8000.196372	13.635175	-0.057408	4.816113
279.081959	8000.328466	13.640179	-0.057371	4.816153
279.025558	8000.433225	13.645184	-0.057361	4.816183
279.199219	8000.264366	13.650189	-0.057393	4.816133
278.962061	8000.455593	13.655194	-0.057349	4.816190
279.014042	8000.059087	13.660199	-0.057359	4.816074
278.944910	8000.358068	13.665203	-0.057346	4.816162
278.927411	8000.456055	13.670208	-0.057343	4.816191
279.071596	8000.018486	13.675213	-0.057370	4.816062
278.962316	8000.343449	13.680218	-0.057350	4.816158
279.048222	8000.164451	13.685223	-0.057366	4.816105
278.972543	8000.118211	13.690227	-0.057352	4.816092
279.055819	8000.159262	13.695232	-0.057367	4.816103
279.237575	8000.155089	13.700237	-0.057401	4.816101
279.042404	8000.528713	13.705242	-0.057365	4.816211
279.085335	8000.135246	13.710247	-0.057373	4.816096
279.033560	8000.333042	13.715251	-0.057364	4.816154
279.221918	8000.314032	13.720256	-0.057399	4.816148
278.949745	8000.030240	13.725261	-0.057348	4.816066
278.954155	8000.455562	13.730266	-0.057349	4.816190
279.084490	8000.195100	13.735271	-0.057373	4.816114
279.044189	8000.348231	13.740275	-0.057366	4.816158
278.975973	8000.497650	13.745280	-0.057353	4.816202
279.017203	8000.253734	13.750285	-0.057361	4.816131
279.138782	8000.414077	13.755290	-0.057384	4.816177
279.105081	8000.200854	13.760295	-0.057377	4.816115
278.944058	8000.279140	13.765299	-0.057348	4.816139
279.097623	8000.208213	13.770304	-0.057376	4.816117
278.894538	7999.975893	13.775309	-0.057338	4.816050
278.768466	8000.382818	13.780314	-0.057315	4.816170
279.203637	8000.281745	13.785319	-0.057396	4.816138
279.004535	8000.124284	13.790323	-0.057359	4.816093
278.825957	8000.285589	13.795328	-0.057326	4.816141
278.931982	8000.189225	13.800333	-0.057346	4.816113
278.802162	8000.012725	13.805338	-0.057322	4.816062
278.848156	7999.956941	13.810343	-0.057330	4.816045
278.895135	8000.240932	13.815347	-0.057339	4.816128
278.826095	8000.288834	13.820352	-0.057326	4.816142
278.796864	8000.415455	13.825357	-0.057321	4.816179
278.650159	8000.512164	13.830362	-0.057294	4.816208
278.934457	8000.417968	13.835367	-0.057347	4.816179
278.807979	8000.304562	13.840371	-0.057323	4.816147
278.770840	8000.332743	13.845376	-0.057317	4.816155
279.046500	8000.378355	13.850381	-0.057368	4.816167
278.911176	8000.427191	13.855386	-0.057343	4.816182
278.732293	8000.129065	13.860391	-0.057310	4.816096
278.762255	8000.409544	13.865395	-0.057315	4.816178
278.930632	8000.171143	13.870400	-0.057347	4.816107
278.888171	8000.110548	13.875405	-0.057339	4.816090
278.883101	8000.437403	13.880410	-0.057338	4.816185
279.037432	7999.975446	13.885415	-0.057367	4.816049
278.907725	8000.200673	13.890419	-0.057343	4.816116
278.861660	8000.196639	13.895424	-0.057334	4.816115
279.010838	7999.964302	13.900429	-0.057362	4.816046
278.945685	8000.354171	13.905434	-0.057350	4.816161
278.995679	8000.076226	13.910439	-0.057359	4.816079
278.988905	8000.126326	13.915443	-0.057358	4.816094
279.000701	8000.200269	13.920448	-0.057360	4.816115
278.907968	8000.034057	13.925453	-0.057343	4.816067
278.850187	8000.390938	13.930458	-0.057333	4.816172
279.106263	8000.111391	13.935463	-0.057380	4.816089
278.895705	8000.195188	13.940467	-0.057341	4.816114
279.051939	8000.357228	13.945472	-0.057371	4.816161
279.421963	8000.223988	13.950477	-0.057439	4.816120
279.253305	8000.312819	13.955482	-0.057408	4.816147
279.067500	8000.270990	13.960487	-0.057374	4.816136
279.135443	8000.291463	13.965491	-0.057386	4.816141
279.285788	7999.882855	13.970496	-0.057414	4.816021
279.100305	7999.958559	13.975501	-0.057380	4.816044
279.065693	8000.312656	13.980506	-0.057374	4.816148
279.152187	8000.257607	13.985511	-0.057390	4.816131
279.246431	8000.143934	13.990515	-0.057407	4.816098
279.048204	8000.125386	13.995520	-0.057370	4.816093
279.232864	8000.025108	14.000525	-0.057405	4.816063
278.998753	8000.296521	14.005530	-0.057361	4.816143
279.163934	8000.065540	14.010535	-0.057392	4.816075
279.058403	8000.112780	14.015539	-0.057373	4.816089
279.033389	8000.344183	14.020544	-0.057368	4.816157
279.048254	8000.200222	14.025549	-0.057371	4.816115
279.027091	8000.199845	14.030554	-0.057367	4.816115
279.173021	8000.154422	14.035559	-0.057394	4.816101
279.037300	8000.024824	14.040563	-0.057369	4.816064
279.045814	8000.265382	14.045568	-0.057371	4.816134
279.191112	8000.123789	14.050573	-0.057398	4.816092
279.157723	8000.322988	14.055578	-0.057392	4.816150
279.160390	7999.854005	14.060583	-0.057392	4.816013
279.046555	8000.058151	14.065587	-0.057371	4.816074
279.216302	8000.236462	14.070592	-0.057403	4.816125
279.051289	7999.912947	14.075597	-0.057372	4.816031
278.898878	8000.412349	14.080602	-0.057344	4.816178
279.069085	8000.287234	14.085607	-0.057376	4.816140
279.184605	8000.135484	14.090611	-0.057397	4.816095
279.145262	8000.374107	14.095616	-0.057390	4.816165
279.119723	8000.201632	14.100621	-0.057385	4.816115
278.958435	8000.475438	14.105626	-0.057356	4.816196
279.051930	8000.156611	14.110631	-0.057373	4.816102
278.932616	8000.429041	14.115635	-0.057351	4.816182
279.019196	8000.319502	14.120640	-0.057367	4.816150
279.052858	7999.939761	14.125645	-0.057373	4.816039
279.014728	8000.303410	14.130650	-0.057366	4.816145
279.209608	8000.142416	14.135655	-0.057403	4.816097
279.360991	8000.133419	14.140659	-0.057431	4.816094
279.106933	8000.377760	14.145664	-0.057384	4.816167
279.198325	8000.203134	14.150669	-0.057401	4.816115
278.831026	8000.450762	14.155674	-0.057333	4.816189
279.134380	8000.331270	14.160679	-0.057389	4.816153
279.056629	8000.487995	14.165683	-0.057375	4.816199
279.106795	8000.265609	14.170688	-0.057384	4.816134
279.180848	8000.119517	14.175693	-0.057398	4.816091
279.026177	8000.553709	14.180698	-0.057369	4.816218
279.120088	8000.333185	14.185703	-0.057387	4.816153
278.991687	8000.327656	14.190707	-0.057363	4.816153
279.277182	8000.400159	14.195712	-0.057416	4.816172
279.205444	8000.216160	14.200717	-0.057403	4.816119
278.994711	8000.297817	14.205722	-0.057364	4.816144
279.128665	8000.088707	14.210727	-0.057389	4.816082
279.128004	8000.316279	14.215731	-0.057389	4.816148
279.109936	8000.479430	14.220736	-0.057386	4.816196
279.241454	8000.225399	14.225741	-0.057410	4.816121
279.032940	8000.398982	14.230746	-0.057371	4.816173
279.016526	8000.344201	14.235751	-0.057368	4.816157
279.028034	8000.268559	14.240755	-0.057371	4.816135
278.997975	8000.339606	14.245760	-0.057365	4.816156
278.999581	8000.450761	14.250765	-0.057366	4.816188
278.953445	8000.609130	14.255770	-0.057357	4.816235
279.154561	8000.440768	14.260775	-0.057395	4.816185
279.195001	8000.392362	14.265779	-0.057402	4.816170
278.968932	8000.566695	14.270784	-0.057360	4.816222
279.067558	8000.428527	14.275789	-0.057379	4.816182
279.133107	7999.531185	14.280794	-0.057390	4.815919

279.267111	7996.276416	14.285799	-0.057413	4.814967
279.291161	7990.700828	14.290803	-0.057414	4.813337
279.223061	7983.953464	14.295808	-0.057397	4.811364
279.055036	7976.705687	14.300813	-0.057361	4.809245
278.779652	7969.023140	14.305818	-0.057305	4.806998
278.822384	7961.246376	14.310823	-0.057308	4.804720
278.878470	7953.404269	14.315827	-0.057313	4.802422
278.778400	7945.401417	14.320832	-0.057290	4.800077
278.911147	7937.453224	14.325837	-0.057309	4.797746
278.500778	7929.437167	14.330842	-0.057228	4.795396
278.431166	7921.399899	14.335847	-0.057209	4.793037
278.650272	7913.389319	14.340851	-0.057245	4.790683
278.670638	7905.415570	14.345856	-0.057244	4.788340
278.563034	7897.417179	14.350861	-0.057219	4.785989
278.550155	7889.428477	14.355866	-0.057211	4.783639
278.569331	7881.450566	14.360871	-0.057210	4.781292
278.526152	7873.436410	14.365875	-0.057196	4.778932
278.351985	7865.435946	14.370880	-0.057159	4.776576
278.380560	7857.422356	14.375885	-0.057159	4.774215
278.348475	7849.389620	14.380890	-0.057148	4.771846
278.400368	7841.398066	14.385895	-0.057152	4.769489
278.169462	7833.403299	14.390899	-0.057104	4.767130
278.235647	7825.355404	14.395904	-0.057111	4.764753
278.219036	7817.422360	14.400909	-0.057103	4.762409
278.100639	7809.371486	14.405914	-0.057076	4.760030
278.084746	7801.472756	14.410919	-0.057068	4.757694
278.104226	7793.363186	14.415923	-0.057066	4.755295
277.795822	7785.309361	14.420928	-0.057004	4.752912
277.824399	7777.310352	14.425933	-0.057004	4.750542
277.727536	7769.364320	14.430938	-0.056981	4.748188
277.757070	7761.323819	14.435943	-0.056981	4.745804
277.855060	7753.380782	14.440947	-0.056994	4.743448
277.962660	7745.341865	14.445952	-0.057009	4.741061
277.686344	7737.371836	14.450957	-0.056953	4.738696
277.447112	7729.338038	14.455962	-0.056903	4.736310
277.668303	7721.330411	14.460967	-0.056939	4.733929
277.461355	7713.316717	14.465971	-0.056895	4.731547
277.327305	7705.321584	14.470976	-0.056865	4.729169
277.507801	7697.339157	14.475981	-0.056894	4.726792
277.459068	7689.324729	14.480986	-0.056879	4.724405
277.475635	7681.381044	14.485991	-0.056877	4.722038
277.310507	7673.350508	14.490995	-0.056842	4.719644
277.342887	7665.342831	14.496000	-0.056842	4.717256
277.234538	7657.332600	14.501005	-0.056817	4.714865
277.072234	7649.273699	14.506010	-0.056782	4.712460
277.063916	7641.321774	14.511015	-0.056775	4.710084
277.011416	7633.298280	14.516019	-0.056760	4.707686
276.901313	7625.295084	14.521024	-0.056735	4.705293
276.931753	7617.422431	14.526029	-0.056735	4.702937
276.829516	7609.267929	14.531034	-0.056711	4.700497
276.883490	7601.362881	14.536039	-0.056716	4.698129
276.769192	7593.301059	14.541043	-0.056689	4.695713
276.743456	7585.280586	14.546048	-0.056679	4.693309
276.660869	7577.275242	14.551053	-0.056659	4.690908
276.517242	7569.269412	14.556058	-0.056627	4.688505
276.674488	7561.275183	14.561063	-0.056651	4.686105
276.635431	7553.310589	14.566067	-0.056639	4.683712
276.475105	7545.307700	14.571072	-0.056604	4.681307
276.595747	7537.352432	14.576077	-0.056621	4.678914
276.554410	7529.268378	14.581082	-0.056608	4.676482
276.329838	7521.252690	14.586087	-0.056561	4.674069
276.442642	7513.216405	14.591091	-0.056577	4.671648
276.346183	7505.222338	14.596096	-0.056554	4.669239
276.425125	7497.227260	14.601101	-0.056564	4.666828
276.294970	7489.212344	14.606106	-0.056534	4.664411
276.199550	7481.273185	14.611111	-0.056511	4.662015
276.117575	7473.227634	14.616115	-0.056491	4.659585
276.136894	7465.253980	14.621120	-0.056489	4.657176
276.247047	7457.241534	14.626125	-0.056505	4.654753
276.116196	7449.215581	14.631130	-0.056475	4.652326
276.047754	7441.203441	14.636135	-0.056457	4.649902
276.053707	7433.283456	14.641139	-0.056453	4.647503
275.962686	7425.217772	14.646144	-0.056431	4.645060
275.847344	7417.311775	14.651149	-0.056405	4.642664
275.673245	7409.194585	14.656154	-0.056367	4.640203
275.603620	7401.250849	14.661159	-0.056349	4.637793
275.669880	7393.219198	14.666163	-0.056356	4.635354
275.488335	7385.208449	14.671168	-0.056317	4.632921
275.496776	7377.161462	14.676173	-0.056314	4.630476
275.561878	7369.213326	14.681178	-0.056321	4.628059
275.710977	7361.196694	14.686183	-0.056343	4.625620
275.572979	7353.244067	14.691187	-0.056313	4.623200
275.379262	7345.193057	14.696192	-0.056271	4.620748
275.592659	7337.218906	14.701197	-0.056306	4.618318
275.349928	7329.174359	14.706202	-0.056256	4.615866
275.367912	7321.170412	14.711207	-0.056254	4.613424
275.198043	7313.191923	14.716211	-0.056217	4.610989
275.044363	7305.161523	14.721216	-0.056183	4.608537
275.031813	7297.183620	14.726221	-0.056176	4.606100
274.863925	7289.178177	14.731226	-0.056139	4.603653
275.011350	7281.190518	14.736231	-0.056162	4.601210
274.992431	7273.228405	14.741235	-0.056153	4.598774
274.728836	7265.186885	14.746240	-0.056099	4.596312
274.796572	7257.204807	14.751245	-0.056106	4.593867
274.665602	7249.123127	14.756250	-0.056077	4.591390
274.752866	7241.123135	14.761255	-0.056088	4.588936
274.691450	7233.139690	14.766259	-0.056071	4.586487
274.753348	7225.134012	14.771264	-0.056078	4.584029
274.595829	7217.145018	14.776269	-0.056043	4.581575
274.497425	7209.137963	14.781274	-0.056020	4.579114
274.586836	7201.130941	14.786279	-0.056031	4.576652
274.394154	7193.173281	14.791283	-0.055990	4.574204
274.354400	7185.101062	14.796288	-0.055978	4.571719
274.364856	7177.129432	14.801293	-0.055974	4.569264
274.256174	7169.131960	14.806298	-0.055949	4.566800
274.240200	7161.151800	14.811303	-0.055941	4.564339
274.208815	7153.143619	14.816307	-0.055930	4.561869
274.062531	7145.148201	14.821312	-0.055898	4.559401
274.203231	7137.195753	14.826317	-0.055919	4.556945
274.181781	7129.140979	14.831322	-0.055910	4.554456
274.125960	7121.100835	14.836327	-0.055894	4.551971
274.121234	7113.125474	14.841331	-0.055888	4.549504
274.199446	7105.099684	14.846336	-0.055897	4.547020
274.166092	7097.114978	14.851341	-0.055886	4.544547
274.124557	7089.139709	14.856346	-0.055873	4.542076
273.854946	7081.162736	14.861351	-0.055818	4.539603
273.976137	7073.185452	14.866355	-0.055835	4.537129
273.790924	7065.107310	14.871360	-0.055796	4.534621
273.731320	7057.107486	14.876365	-0.055779	4.532137
273.793305	7049.084337	14.881370	-0.055786	4.529644
273.787246	7041.123178	14.886375	-0.055780	4.527170
273.781102	7033.089116	14.891379	-0.055773	4.524671
273.611725	7025.149686	14.896384	-0.055737	4.522200
273.536166	7017.149970	14.901389	-0.055717	4.519709
273.607078	7009.128770	14.906394	-0.055726	4.517210
273.392744	7001.129791	14.911399	-0.055680	4.514716
273.323883	6993.065339	14.916403	-0.055662	4.512201
273.316504	6985.047017	14.921408	-0.055656	4.509698
273.477899	6977.094977	14.926413	-0.055681	4.507216
273.292276	6969.006840	14.931418	-0.055641	4.504688
273.341510	6961.116330	14.936423	-0.055645	4.502222
273.151721	6953.073236	14.941427	-0.055605	4.499706
273.120748	6945.104326	14.946432	-0.055594	4.497212
273.168790	6937.090397	14.951437	-0.055598	4.494703
272.963676	6929.047094	14.956442	-0.055554	4.492183
272.882612	6921.048200	14.961447	-0.055534	4.489675
273.056761	6913.082520	14.966451	-0.055561	4.487177
273.020611	6905.028539	14.971456	-0.055549	4.484650
272.797413	6897.121914	14.976461	-0.055503	4.482166
272.555005	6889.074896	14.981466	-0.055453	4.479637
272.649388	6881.091985	14.986471	-0.055465	4.477128
272.660507	6873.065677	14.991475	-0.055462	4.474604
272.563205	6865.042957	14.996480	-0.055439	4.472079
272.659296	6857.043741	15.001485	-0.055451	4.469560
272.545729	6849.042177	15.006490	-0.055425	4.467039
272.530248	6840.988743	15.011495	-0.055417	4.464500
272.348751	6833.046512	15.016499	-0.055378	4.461994
272.306650	6824.993622	15.021504	-0.055365	4.459453
272.491451	6817.068435	15.026509	-0.055394	4.456951
272.362755	6809.025608	15.031514	-0.055365	4.454409
272.538146	6801.034396	15.036519	-0.055393	4.451883
272.268457	6792.997444	15.041523	-0.055338	4.449340
272.054830	6785.020766	15.046528	-0.055293	4.446815
272.153250	6777.074622	15.051533	-0.055306	4.444299
271.998471	6769.051253	15.056538	-0.055272	4.441756
271.940954	6761.054013	15.061543	-0.055256	4.439220
271.924060	6753.022501	15.066547	-0.055248	4.436672
271.952259	6744.966539	15.071552	-0.055248	4.434116
272.075050	6736.966104	15.076557	-0.055266	4.431575
271.977346	6728.976006	15.081562	-0.055242	4.429036
271.931774	6720.979057	15.086567	-0.055229	4.426493
272.002560	6713.016578	15.091571	-0.055237	4.423960
271.827241	6704.970771	15.096576	-0.055199	4.421398
271.840825	6697.033932	15.101581	-0.055196	4.418870
271.686665	6688.960980	15.106586	-0.055162	4.416297
271.650125	6680.995877	15.111591	-0.055150	4.413757
271.720075	6672.980062	15.116595	-0.055158	4.411199
271.619879	6664.968402	15.121600	-0.055135	4.408641
271.585521	6656.993696	15.126605	-0.055123	4.406094
271.268510	6648.966301	15.131610	-0.055059	4.403526
271.327282	6640.978082	15.136615	-0.055065	4.400972
271.411924	6633.031155	15.141619	-0.055075	4.398429
271.268276	6624.993866	15.146624	-0.055043	4.395855
271.301402	6617.042371	15.151629	-0.055044	4.393308
271.203865	6608.944687	15.156634	-0.055021	4.390712
271.238830	6600.991786	15.161639	-0.055023	4.388161
271.044334	6592.968450	15.166643	-0.054981	4.385585
271.170708	6584.992273	15.171648	-0.055000	4.383025
270.981498	6577.000700	15.176653	-0.054959	4.380456
270.833080	6569.023891	15.181658	-0.054926	4.377890
270.890767	6560.986229	15.186663	-0.054932	4.375305
270.830244	6553.009635	15.191667	-0.054916	4.372737
270.724227	6544.954240	15.196672	-0.054891	4.370142
270.717067	6537.008477	15.201677	-0.054884	4.367582
270.803708	6528.954406	15.206682	-0.054895	4.364985
270.879728	6521.053295	15.211687	-0.054904	4.362436
270.582101	6513.011783	15.216691	-0.054844	4.359838
270.576061	6505.015249	15.221696	-0.054837	4.357255
270.668074	6496.998473	15.226701	-0.054849	4.354665
270.601457	6488.876503	15.231706	-0.054832	4.352037
270.439057	6480.927175	15.236711	-0.054797	4.349464
270.575795	6472.961475	15.241715	-0.054817	4.346886
270.496789	6464.928525	15.246720	-0.054797	4.344282
270.417204	6457.023671	15.251725	-0.054777	4.341719
270.368185	6448.956468	15.256730	-0.054763	4.339102
270.321454	6440.923923	15.261735	-0.054749	4.336495
270.330938	6432.960453	15.266739	-0.054746	4.333908
270.385080	6424.902871	15.271744	-0.054751	4.331290
270.263425	6416.959334	15.276749	-0.054723	4.328706
269.916778	6408.948515	15.281754	-0.054653	4.326098
270.030268	6400.978116	15.286759	-0.054669	4.323504
270.115759	6392.991017	15.291763	-0.054680	4.320902
269.970691	6384.992544	15.296768	-0.054648	4.318294
269.983553	6376.932419	15.301773	-0.054645	4.315665
269.811111	6368.903222	15.306778	-0.054608	4.313044
269.837499	6360.915732	15.311783	-0.054607	4.310436
269.619299	6352.950890	15.316787	-0.054562	4.307832
269.498673	6344.915283	15.321792	-0.054534	4.305204
269.796977	6336.979216	15.326797	-0.054585	4.302610
269.547783	6328.932467	15.331802	-0.054533	4.299974
269.629720	6320.957515	15.336807	-0.054543	4.297362
269.654409	6312.931569	15.341811	-0.054543	4.294732
269.470736	6304.892542	15.346816	-0.054503	4.292094
269.662148	6296.904909	15.351821	-0.054534	4.289474
269.398388	6288.932846	15.356826	-0.054479	4.286855
269.493742	6280.926813	15.361831	-0.054492	4.284225
269.311204	6272.922849	15.366835	-0.054453	4.281592
269.459949	6264.954765	15.371840	-0.054476	4.278972
269.466296	6256.952317	15.376845	-0.054472	4.276338
269.157620	6248.931288	15.381850	-0.054409	4.273694
269.144061	6240.874890	15.386855	-0.054401	4.271039
269.100948	6232.864004	15.391859	-0.054388	4.268396
268.933361	6224.884885	15.396864	-0.054352	4.265762
268.674525	6216.905527	15.401869	-0.054298	4.263125
268.636469	6208.909510	15.406874	-0.054286	4.260483
268.698581	6200.917781	15.411879	-0.054293	4.257842
268.675464	6192.927548	15.416883	-0.054283	4.255198
268.617012	6184.882877	15.421888	-0.054267	4.252535
268.811814	6176.892194	15.426893	-0.054298	4.249890
268.678562	6168.923605	15.431898	-0.054268	4.247248
268.450807	6160.896688	15.436903	-0.054221	4.244584
268.557149	6152.955253	15.441907	-0.054236	4.241949
268.540993	6144.907371	15.446912	-0.054227	4.239277
268.444843	6136.967274	15.451917	-0.054204	4.236638
268.204965	6128.930990	15.456922	-0.054155	4.233964
268.381531	6120.873327	15.461927	-0.054182	4.231285
268.081083	6112.949347	15.466931	-0.054121	4.228644
267.960588	6104.898895	15.471936	-0.054094	4.225962
268.246876	6096.967563	15.476941	-0.054142	4.223321
268.009090	6088.925019	15.481946	-0.054092	4.220636
267.966574	6080.990572	15.486951	-0.054079	4.217988
268.054115	6072.934007	15.491955	-0.054091	4.215298
268.109719	6064.907769	15.496960	-0.054096	4.212617
268.010925	6056.892084	15.501965	-0.054072	4.209935
267.883303	6048.924379	15.506970	-0.054043	4.207268
267.895101	6040.906376	15.511975	-0.054040	4.204584
267.943386	6032.987430	15.516979	-0.054044	4.201932
267.720478	6024.953150	15.521984	-0.053998	4.199236
267.807151	6016.972439	15.526989	-0.054009	4.196560
267.588128	6008.890810	15.531994	-0.053963	4.193845
267.470486	6000.841137	15.536999	-0.053936	4.191140
267.538708	5992.877341	15.542003	-0.053943	4.188464
267.539021	5984.854834	15.547008	-0.053938	4.185766
267.419909	5976.925635	15.552013	-0.053911	4.183097
267.202562	5968.859132	15.557018	-0.053865	4.180378
267.257914	5960.927350	15.562023	-0.053870	4.177706
267.299505	5952.892768	15.567027	-0.053873	4.174997
267.171854	5944.888239	15.572032	-0.053844	4.172295
267.291657	5936.888374	15.577037	-0.053861	4.169595
267.235607	5928.898427	15.582042	-0.053846	4.166896
267.271318	5920.874690	15.587047	-0.053847	4.164183
267.180701	5912.933205	15.592051	-0.053825	4.161496
267.147008	5904.888063	15.597056	-0.053814	4.158772
267.032447	5896.931060	15.602061	-0.053787	4.156076
266.720763	5888.893779	15.607066	-0.053724	4.153348
266.842779	5880.852865	15.612071	-0.053742	4.150622
266.897578	5872.906822	15.617075	-0.053747	4.147926
266.782886	5864.837520	15.622080	-0.053720	4.145184
266.520030	5856.936637	15.627085	-0.053666	4.142496
266.712836	5848.887665	15.632090	-0.053697	4.139762
266.608563	5840.940426	15.637095	-0.053672	4.137056
266.575372	5832.894226	15.642099	-0.053661	4.134316
266.415564	5824.870632	15.647104	-0.053626	4.131580
266.496596	5816.899794	15.652109	-0.053636	4.128863
266.256542	5808.898877	15.657114	-0.053586	4.126131
266.450496	5800.910791	15.662119	-0.053617	4.123406
266.530498	5792.927418	15.667123	-0.053627	4.120679
266.392658	5784.892316	15.672128	-0.053596	4.117931
266.430474	5776.918332	15.677133	-0.053598	4.115203
266.306947	5768.836055	15.682138	-0.053570	4.112435
266.192467	5760.810881	15.687143	-0.053543	4.109684
266.144403	5752.882474	15.692147	-0.053529	4.106966
266.174452	5744.851824	15.697152	-0.053530	4.104212
266.138083	5736.905403	15.702157	-0.053518	4.101484
266.026334	5728.923488	15.707162	-0.053492	4.098741
265.885150	5720.908120	15.712167	-0.053461	4.095984
266.045899	5712.931296	15.717171	-0.053485	4.093243
265.774630	5704.896328	15.722176	-0.053430	4.090474
265.693227	5696.942152	15.727181	-0.053410	4.087733
265.906573	5688.877926	15.732186	-0.053444	4.084957
265.790282	5680.958480	15.737191	-0.053417	4.082224
265.674607	5672.975637	15.742195	-0.053391	4.079468
265.619601	5664.957026	15.747200	-0.053375	4.076698
265.501927	5656.946344	15.752205	-0.053348	4.073928
265.404603	5648.915096	15.757210	-0.053325	4.071150
265.339407	5640.925991	15.762215	-0.053308	4.068384
265.419617	5632.913154	15.767219	-0.053317	4.065611
265.336151	5624.942003	15.772224	-0.053297	4.062847
265.306874	5616.930045	15.777229	-0.053286	4.060069
265.271308	5608.956223	15.782234	-0.053274	4.057301
265.098992	5600.935869	15.787239	-0.053237	4.054514
264.908947	5592.920932	15.792243	-0.053197	4.051726
264.955988	5584.901021	15.797248	-0.053200	4.048938
265.268105	5576.910730	15.802253	-0.053253	4.046163
265.051591	5568.958341	15.807258	-0.053208	4.043391
264.942498	5560.921067	15.812263	-0.053182	4.040589
264.818118	5552.984937	15.817267	-0.053154	4.037820
264.849939	5544.919871	15.822272	-0.053155	4.035006
264.658152	5536.818866	15.827277	-0.053114	4.032175
264.761576	5528.857671	15.832282	-0.053128	4.029395
264.871527	5520.857920	15.837287	-0.053143	4.026599
264.851089	5512.918297	15.842291	-0.053135	4.023821
264.822931	5504.893584	15.847296	-0.053124	4.021011
264.658411	5496.921333	15.852301	-0.053088	4.018215
264.649263	5488.907055	15.857306	-0.053082	4.015405
264.526314	5480.891770	15.862311	-0.053054	4.012591
264.528171	5472.891841	15.867315	-0.053049	4.009782
264.295743	5464.882904	15.872320	-0.053000	4.006964
264.412627	5456.900746	15.877325	-0.053017	4.004160
264.436160	5448.898103	15.882330	-0.053016	4.001344
264.466428	5440.902563	15.887335	-0.053017	3.998529
264.448862	5432.928063	15.892339	-0.053008	3.995719
264.207916	5424.897486	15.897344	-0.052958	3.992884
264.242553	5416.888645	15.902349	-0.052960	3.990058
264.146443	5408.907278	15.907354	-0.052937	3.987239
264.021900	5400.905513	15.912359	-0.052908	3.984409
264.121642	5392.940766	15.917363	-0.052922	3.981594
263.959858	5384.920367	15.922368	-0.052886	3.978754
263.938812	5376.952191	15.927373	-0.052877	3.975932
264.053696	5368.927939	15.932378	-0.052894	3.973090
263.980344	5360.889057	15.937383	-0.052875	3.970238
263.830315	5352.930787	15.942387	-0.052842	3.967411
263.565817	5344.915057	15.947392	-0.052787	3.964560
263.879710	5336.986115	15.952397	-0.052841	3.961748
263.592005	5328.954097	15.957402	-0.052782	3.958886
263.539030	5320.961643	15.962407	-0.052767	3.956041
263.477860	5312.967472	15.967411	-0.052750	3.953193
263.424604	5304.927931	15.972416	-0.052735	3.950327
263.345726	5296.970730	15.977421	-0.052716	3.947487
263.295282	5288.928744	15.982426	-0.052701	3.944616
263.436963	5280.980358	15.987431	-0.052722	3.941779
263.273151	5272.993065	15.992435	-0.052687	3.938921
263.223827	5264.967691	15.997440	-0.052672	3.936050
263.385471	5256.974517	16.002445	-0.052697	3.933191
263.252493	5248.950134	16.007450	-0.052667	3.930314
263.098467	5240.973642	16.012455	-0.052634	3.927452
263.148115	5232.979925	16.017459	-0.052638	3.924585
262.936799	5225.031928	16.022464	-0.052593	3.921728
262.999052	5217.014523	16.027469	-0.052600	3.918848
262.910481	5209.012267	16.032474	-0.052578	3.915970
262.715453	5200.983988	16.037479	-0.052537	3.913077
262.651345	5192.998474	16.042483	-0.052520	3.910201
262.608377	5184.953712	16.047488	-0.052506	3.907301
262.770655	5176.981548	16.052493	-0.052531	3.904429
262.514040	5168.988976	16.057498	-0.052479	3.901540
262.618018	5160.974485	16.062503	-0.052493	3.898647
262.755773	5153.009934	16.067507	-0.052513	3.895771
262.557331	5144.961552	16.072512	-0.052471	3.892857
262.730686	5136.945745	16.077517	-0.052498	3.889959
262.370049	5129.002355	16.082522	-0.052426	3.887074
262.491058	5120.979642	16.087527	-0.052443	3.884168
262.468436	5113.012559	16.092531	-0.052434	3.881278
262.250357	5105.028170	16.097536	-0.052388	3.878375
262.351782	5097.016692	16.102541	-0.052402	3.875466
262.151364	5088.814303	16.107546	-0.052360	3.872480
262.120699	5080.832308	16.112551	-0.052349	3.869575
262.144354	5072.899711	16.117555	-0.052348	3.866687
261.999495	5064.923820	16.122560	-0.052316	3.863777
261.977844	5056.941398	16.127565	-0.052307	3.860866
261.788769	5048.993705	16.132570	-0.052266	3.857961
261.729924	5040.971559	16.137575	-0.052250	3.855030
261.821381	5033.008859	16.142579	-0.052262	3.852121
261.842945	5024.977460	16.147584	-0.052261	3.849184
261.877932	5016.995784	16.152589	-0.052263	3.846263
261.836302	5009.003073	16.157594	-0.052250	3.843334
261.613170	5001.002641	16.162599	-0.052203	3.840396
261.446106	4993.083584	16.167603	-0.052167	3.837487
261.406309	4985.030972	16.172608	-0.052154	3.834529
261.466509	4977.024039	16.177613	-0.052160	3.831588
261.459582	4968.988799	16.182618	-0.052154	3.828632
261.333290	4961.000380	16.187623	-0.052125	3.825690
261.286613	4953.079776	16.192627	-0.052111	3.822771
261.155972	4945.046382	16.197632	-0.052082	3.819807
261.149075	4937.129865	16.202637	-0.052076	3.816887
261.126216	4929.080850	16.207642	-0.052066	3.813914
261.094120	4921.051323	16.212647	-0.052055	3.810947
260.963962	4913.081787	16.217651	-0.052026	3.807997
261.029557	4905.038099	16.222656	-0.052033	3.805022
260.938111	4897.131069	16.227661	-0.052011	3.802092
260.821566	4889.119645	16.232666	-0.051984	3.799120
260.792931	4881.081685	16.237671	-0.051973	3.796138
260.913284	4873.074176	16.242675	-0.051991	3.793168
260.851450	4865.007929	16.247680	-0.051974	3.790170
260.791374	4857.083130	16.252685	-0.051958	3.787222
260.726507	4849.052430	16.257690	-0.051940	3.784232
260.693632	4841.080696	16.262695	-0.051929	3.781263
260.766668	4833.096418	16.267699	-0.051938	3.778289
260.626903	4825.079994	16.272704	-0.051906	3.775296
260.627542	4817.061633	16.277709	-0.051901	3.772303
260.475552	4809.079646	16.282714	-0.051868	3.769317
260.348530	4801.105063	16.287719	-0.051839	3.766333
260.267913	4793.113220	16.292723	-0.051819	3.763341
260.066058	4785.119256	16.297728	-0.051776	3.760343
260.220274	4777.130193	16.302733	-0.051800	3.757352
260.217439	4769.101219	16.307738	-0.051794	3.754341
260.137713	4761.071741	16.312743	-0.051774	3.751325
260.034996	4753.084225	16.317747	-0.051750	3.748322
260.268989	4745.064256	16.322752	-0.051788	3.745312
260.075640	4737.125026	16.327757	-0.051747	3.742320
259.902474	4729.123037	16.332762	-0.051710	3.739303
259.809964	4721.138330	16.337767	-0.051688	3.736291
259.924318	4713.123268	16.342771	-0.051704	3.733271
259.710550	4705.089621	16.347776	-0.051659	3.730233
259.680653	4697.135382	16.352781	-0.051648	3.727227
259.636672	4689.140591	16.357786	-0.051635	3.724203
259.761702	4681.151589	16.362791	-0.051653	3.721183
259.677074	4673.205319	16.367795	-0.051632	3.718172
259.559849	4665.163853	16.372800	-0.051605	3.715121
259.597911	4657.096985	16.377805	-0.051607	3.712062
259.419364	4649.127810	16.382810	-0.051569	3.709032
259.522940	4641.123400	16.387815	-0.051583	3.705993
259.485068	4633.141961	16.392819	-0.051571	3.702957
259.184475	4625.147071	16.397824	-0.051509	3.699906
259.217095	4617.212814	16.402829	-0.051510	3.696885
259.236556	4609.183562	16.407834	-0.051509	3.693824
259.453454	4601.152252	16.412839	-0.051544	3.690765
259.354040	4593.216726	16.417843	-0.051521	3.687733
259.189821	4585.188300	16.422848	-0.051485	3.684660
259.209155	4577.240310	16.427853	-0.051483	3.681621
258.918794	4569.240940	16.432858	-0.051424	3.678551
258.916117	4561.241669	16.437863	-0.051418	3.675486
258.861013	4553.243587	16.442867	-0.051403	3.672418
258.804637	4545.219777	16.447872	-0.051387	3.669337
258.910664	4537.233391	16.452877	-0.051402	3.666272
258.791907	4529.232891	16.457882	-0.051375	3.663194
258.637564	4521.212352	16.462887	-0.051341	3.660104
258.695910	4513.278424	16.467891	-0.051347	3.657050
258.446632	4505.247876	16.472896	-0.051295	3.653949
258.565038	4497.220530	16.477901	-0.051312	3.650856
258.465217	4489.243784	16.482906	-0.051288	3.647774
258.432858	4481.214339	16.487911	-0.051277	3.644670
258.634626	4473.299312	16.492915	-0.051310	3.641615
258.212014	4465.285837	16.497920	-0.051226	3.638502
258.241309	4457.321037	16.502925	-0.051226	3.635418
258.142663	4449.263095	16.507930	-0.051203	3.632291
258.101962	4441.214592	16.512935	-0.051190	3.629167
258.124593	4433.222515	16.517939	-0.051189	3.626063
257.918151	4425.273982	16.522944	-0.051145	3.622968
258.077998	4417.285293	16.527949	-0.051170	3.619865
257.996431	4409.355435	16.532954	-0.051150	3.616775
257.776874	4401.284261	16.537959	-0.051104	3.613624
257.833753	4393.297719	16.542963	-0.051109	3.610510
257.667076	4385.305738	16.547968	-0.051073	3.607385
257.786120	4377.305471	16.552973	-0.051090	3.604263
257.696171	4369.330012	16.557978	-0.051068	3.601141
257.529263	4361.358980	16.562983	-0.051032	3.598017
257.785823	4353.380873	16.567987	-0.051075	3.594899
257.693392	4345.321361	16.572992	-0.051052	3.591736
257.628728	4337.344946	16.577997	-0.051035	3.588604
257.663362	4329.366846	16.583002	-0.051036	3.585471
257.570700	4321.365932	16.588007	-0.051014	3.582324
257.476772	4313.404706	16.593011	-0.050991	3.579188
257.599856	4305.395250	16.598016	-0.051009	3.576038
257.276868	4297.413941	16.603021	-0.050944	3.572883
257.110910	4289.381000	16.608026	-0.050908	3.569709
257.193610	4281.420206	16.613031	-0.050918	3.566568
257.282827	4273.401171	16.618035	-0.050930	3.563401
256.974051	4265.393834	16.623040	-0.050867	3.560225
257.078976	4257.475425	16.628045	-0.050881	3.557093
257.033170	4249.395463	16.633050	-0.050868	3.553890
256.938442	4241.318545	16.638055	-0.050845	3.550683
256.859886	4233.389271	16.643059	-0.050825	3.547533
256.830992	4225.350313	16.648064	-0.050815	3.544338
256.716756	4217.412836	16.653069	-0.050788	3.541178
256.676285	4209.418217	16.658074	-0.050776	3.537995
256.805273	4201.398599	16.663079	-0.050794	3.534803
256.633532	4193.446218	16.668083	-0.050757	3.531627
256.471814	4185.414323	16.673088	-0.050722	3.528416
256.375139	4177.414611	16.678093	-0.050699	3.525217
256.203355	4169.481718	16.683098	-0.050662	3.522040
256.269207	4161.484314	16.688103	-0.050669	3.518841
256.403019	4153.516274	16.693107	-0.050689	3.515654
256.117427	4145.464288	16.698112	-0.050630	3.512416
256.169866	4137.451664	16.703117	-0.050635	3.509202
256.008219	4129.496885	16.708122	-0.050600	3.506002
256.141386	4121.473334	16.713127	-0.050619	3.502780
256.096642	4113.509530	16.718131	-0.050606	3.499574
255.937515	4105.530861	16.723136	-0.050571	3.496355
255.964802	4097.533632	16.728141	-0.050571	3.493131
255.943805	4089.506527	16.733146	-0.050562	3.489891
255.902413	4081.550277	16.738151	-0.050549	3.486676
255.958588	4073.570653	16.743155	-0.050555	3.483452
255.712162	4065.571074	16.748160	-0.050504	3.480207
256.000537	4057.605108	16.753165	-0.050552	3.476989
255.653870	4049.577569	16.758170	-0.050483	3.473724
255.585087	4041.550548	16.763175	-0.050465	3.470464
255.440078	4033.587805	16.768179	-0.050432	3.467225
255.394411	4025.565643	16.773184	-0.050419	3.463962
255.589442	4017.599512	16.778189	-0.050450	3.460726
255.609535	4009.614010	16.783194	-0.050449	3.457474
255.270060	4001.612542	16.788199	-0.050380	3.454201
255.272519	3993.620643	16.793203	-0.050376	3.450939
255.323561	3985.610272	16.798208	-0.050380	3.447668
255.199559	3977.633704	16.803213	-0.050352	3.444403
255.162398	3969.628823	16.808218	-0.050340	3.441125
255.253532	3961.668498	16.813223	-0.050352	3.437867
255.271265	3953.653872	16.818227	-0.050350	3.434581
254.945255	3945.645044	16.823232	-0.050284	3.431283
254.927045	3937.652556	16.828237	-0.050275	3.427999
254.862213	3929.657110	16.833242	-0.050258	3.424709
254.782009	3921.674424	16.838247	-0.050238	3.421420
254.876646	3913.716240	16.843251	-0.050251	3.418144
255.003892	3905.663108	16.848256	-0.050269	3.414827
254.897316	3897.685291	16.853261	-0.050244	3.411530
254.640985	3889.731324	16.858266	-0.050191	3.408234
254.790133	3881.700475	16.863271	-0.050214	3.404917
254.694128	3873.779023	16.868275	-0.050191	3.401634
254.418888	3865.755870	16.873280	-0.050135	3.398300
254.513142	3857.780026	16.878285	-0.050147	3.394994
254.520408	3849.679375	16.883290	-0.050143	3.391630
254.428810	3841.681332	16.888295	-0.050121	3.388303
254.391621	3833.736896	16.893299	-0.050109	3.384996
254.476562	3825.749559	16.898304	-0.050120	3.381672
254.567225	3817.766566	16.903309	-0.050131	3.378347
254.365904	3809.814462	16.908314	-0.050089	3.375022
254.242448	3801.786788	16.913319	-0.050061	3.371664
254.188043	3793.821038	16.918323	-0.050045	3.368331
254.200099	3785.796439	16.923328	-0.050042	3.364973
253.989409	3777.864304	16.928333	-0.049998	3.361642
254.126717	3769.855460	16.933338	-0.050019	3.358288
254.041590	3761.842311	16.938343	-0.049998	3.354921
253.954346	3753.850056	16.943347	-0.049976	3.351559
253.970940	3745.861418	16.948352	-0.049974	3.348199
253.770135	3737.874272	16.953357	-0.049932	3.344829
253.614503	3729.907674	16.958362	-0.049898	3.341465
253.688258	3721.897586	16.963367	-0.049906	3.338088
253.672197	3713.897429	16.968371	-0.049898	3.334708
253.502883	3705.887678	16.973376	-0.049861	3.331316
253.462066	3697.917035	16.978381	-0.049849	3.327941
253.442999	3689.937141	16.983386	-0.049840	3.324559
253.223051	3681.977756	16.988391	-0.049794	3.321176
253.381312	3673.985433	16.993395	-0.049818	3.317789
253.171683	3665.989385	16.998400	-0.049774	3.314383
253.084952	3657.955657	17.003405	-0.049753	3.310962
253.034252	3649.971805	17.008410	-0.049738	3.307560
252.942124	3641.960321	17.013415	-0.049716	3.304142
253.173350	3633.997323	17.018419	-0.049754	3.300753
252.889661	3626.023011	17.023424	-0.049696	3.297336
252.780161	3618.019745	17.028429	-0.049670	3.293909
252.739102	3610.020959	17.033434	-0.049658	3.290484
252.747609	3602.052319	17.038439	-0.049654	3.287070
252.684072	3594.068574	17.043443	-0.049637	3.283642
252.451604	3586.085805	17.048448	-0.049589	3.280206
252.751696	3578.102904	17.053453	-0.049639	3.276786
252.661798	3570.075540	17.058458	-0.049618	3.273328
252.592749	3562.049755	17.063463	-0.049600	3.269869
252.772420	3554.093243	17.068467	-0.049628	3.266445
252.562209	3546.091386	17.073472	-0.049584	3.262982
252.477089	3538.128657	17.078477	-0.049563	3.259538
252.275107	3530.185739	17.083482	-0.049520	3.256094
252.125060	3522.142832	17.088487	-0.049487	3.252605
252.130454	3514.150575	17.093491	-0.049483	3.249141
252.126352	3506.146863	17.098496	-0.049477	3.245667
252.210731	3498.170182	17.103501	-0.049487	3.242205
252.098219	3490.204299	17.108506	-0.049461	3.238737
251.960825	3482.221349	17.113511	-0.049431	3.235255
251.972947	3474.163098	17.118515	-0.049428	3.231744
251.798936	3466.163005	17.123520	-0.049390	3.228246
251.805293	3458.179952	17.128525	-0.049386	3.224760
251.816733	3450.234318	17.133530	-0.049383	3.221286
251.791237	3442.235112	17.138535	-0.049373	3.217783
251.737614	3434.247968	17.143539	-0.049358	3.214281
251.682160	3426.252660	17.148544	-0.049343	3.210771
251.777368	3418.266220	17.153549	-0.049355	3.207268
251.648763	3410.294569	17.158554	-0.049326	3.203758
251.494604	3402.311440	17.163559	-0.049293	3.200238
251.566822	3394.388774	17.168563	-0.049301	3.196750
251.393608	3386.362797	17.173568	-0.049263	3.193202
251.190603	3378.338050	17.178573	-0.049221	3.189650
251.378997	3370.344508	17.183578	-0.049250	3.186124
251.159002	3362.375980	17.188583	-0.049204	3.182588
251.024892	3354.405423	17.193587	-0.049174	3.179051
251.077486	3346.363383	17.198592	-0.049179	3.175486
251.197709	3338.385717	17.203597	-0.049196	3.171948
251.224813	3330.373178	17.208602	-0.049196	3.168387
250.844506	3322.405951	17.213607	-0.049120	3.164825
250.966695	3314.487774	17.218611	-0.049138	3.161302
250.905633	3306.477818	17.223616	-0.049121	3.157726
250.786139	3298.500779	17.228621	-0.049094	3.154159
250.725708	3290.430103	17.233626	-0.049078	3.150548
250.684840	3282.444192	17.238631	-0.049065	3.146972
250.770279	3274.494101	17.243635	-0.049076	3.143413
250.432367	3266.517693	17.248640	-0.049008	3.139820
250.548103	3258.541753	17.253645	-0.049024	3.136243
250.522356	3250.547055	17.258650	-0.049014	3.132647
250.419850	3242.536495	17.263655	-0.048990	3.129036
250.384506	3234.559105	17.268659	-0.048978	3.125439
250.333660	3226.594518	17.273664	-0.048964	3.121843
250.315775	3218.621383	17.278669	-0.048955	3.118241
250.239482	3210.629434	17.283674	-0.048936	3.114623
250.437731	3202.596908	17.288679	-0.048967	3.110995
250.409615	3194.620187	17.293683	-0.048957	3.107378
250.343972	3186.624185	17.298688	-0.048940	3.103746
250.276385	3178.667299	17.303693	-0.048922	3.100128
249.996091	3170.725861	17.308698	-0.048865	3.096502
249.877195	3162.712658	17.313703	-0.048838	3.092848
249.944546	3154.698556	17.318707	-0.048845	3.089196
250.046229	3146.688403	17.323712	-0.048859	3.085544
249.893029	3138.752894	17.328717	-0.048825	3.081910
249.775364	3130.791882	17.333722	-0.048798	3.078262
249.767172	3122.766670	17.338727	-0.048791	3.074585
249.742363	3114.698328	17.343731	-0.048782	3.070883
249.568078	3106.746587	17.348736	-0.048744	3.067223
249.560299	3098.782782	17.353741	-0.048737	3.063561
249.670195	3090.791465	17.358746	-0.048753	3.059887
249.466013	3082.833559	17.363751	-0.048710	3.056210
249.541599	3074.839207	17.368755	-0.048719	3.052524
249.542001	3066.820967	17.373760	-0.048714	3.048819
249.464393	3058.860260	17.378765	-0.048694	3.045133
249.312260	3050.934400	17.383770	-0.048661	3.041455
249.169546	3042.937168	17.388775	-0.048629	3.037740
249.235562	3034.945090	17.393779	-0.048636	3.034033
248.974465	3026.930737	17.398784	-0.048582	3.030295
248.962475	3018.965003	17.403789	-0.048575	3.026587
249.093730	3010.971433	17.408794	-0.048594	3.022868
248.900326	3002.973186	17.413799	-0.048553	3.019127
248.863482	2995.020100	17.418803	-0.048541	3.015410
248.858014	2987.002196	17.423808	-0.048535	3.011660
248.911190	2979.026137	17.428813	-0.048540	3.007927
248.825723	2971.035195	17.433818	-0.048519	3.004176
248.713768	2963.089618	17.438823	-0.048493	3.000440
248.876093	2955.133833	17.443827	-0.048518	2.996708
248.484708	2947.128110	17.448832	-0.048440	2.992921
248.508676	2939.106177	17.453837	-0.048439	2.989142
248.457649	2931.133372	17.458842	-0.048425	2.985377
248.521931	2923.142607	17.463847	-0.048431	2.981605
248.498102	2915.191045	17.468851	-0.048422	2.977843
248.493035	2907.193539	17.473856	-0.048416	2.974054
248.374062	2899.187420	17.478861	-0.048388	2.970251
248.264531	2891.237918	17.483866	-0.048363	2.966471
248.004870	2883.254918	17.488871	-0.048309	2.962662
248.133972	2875.292526	17.493875	-0.048328	2.958878
248.003512	2867.319624	17.498880	-0.048299	2.955071
247.938300	2859.290583	17.503885	-0.048282	2.951235
247.890221	2851.298897	17.508890	-0.048268	2.947413
247.777086	2843.316134	17.513895	-0.048241	2.943587
247.754119	2835.365335	17.518899	-0.048232	2.939776
247.778096	2827.393124	17.523904	-0.048231	2.935952
247.822352	2819.368048	17.528909	-0.048234	2.932099
247.708434	2811.392058	17.533914	-0.048208	2.928256
247.577604	2803.405121	17.538919	-0.048179	2.924402
247.784523	2795.440527	17.543923	-0.048212	2.920571
247.673850	2787.495716	17.548928	-0.048186	2.916728
247.555388	2779.433259	17.553933	-0.048159	2.912823
247.615427	2771.427212	17.558938	-0.048165	2.908949
247.293705	2763.465936	17.563943	-0.048100	2.905072
247.419754	2755.515113	17.568947	-0.048119	2.901218
247.333243	2747.545556	17.573952	-0.048097	2.897339
247.201595	2739.567986	17.578957	-0.048068	2.893448
246.992385	2731.572024	17.583962	-0.048024	2.889538
246.875819	2723.596560	17.588967	-0.047997	2.885639
246.983929	2715.636402	17.593971	-0.048012	2.881753
246.798509	2707.669791	17.598976	-0.047972	2.877844
246.859254	2699.656816	17.603981	-0.047978	2.873919
246.809936	2691.644768	17.608986	-0.047964	2.869984
246.632379	2683.677089	17.613991	-0.047926	2.866058
246.777716	2675.717289	17.618995	-0.047948	2.862148
246.682973	2667.734402	17.624000	-0.047925	2.858209
246.584863	2659.770537	17.629005	-0.047902	2.854273
246.613095	2651.780156	17.634010	-0.047902	2.850325
246.486029	2643.803180	17.639015	-0.047873	2.846370
246.554854	2635.839193	17.644019	-0.047881	2.842427
246.358000	2627.883540	17.649024	-0.047839	2.838468
246.225528	2619.901678	17.654029	-0.047809	2.834494
246.194847	2611.871904	17.659034	-0.047798	2.830496
246.178977	2603.891872	17.664039	-0.047790	2.826518
246.269646	2595.929719	17.669043	-0.047802	2.822549
246.016037	2587.961758	17.674048	-0.047750	2.818552
246.075017	2579.973927	17.679053	-0.047755	2.814557
245.988682	2571.999077	17.684058	-0.047734	2.810555
245.989438	2564.007014	17.689063	-0.047729	2.806544
246.075007	2556.027198	17.694067	-0.047740	2.802538
245.880899	2548.065469	17.699072	-0.047699	2.798519
245.732919	2540.113069	17.704077	-0.047666	2.794501
245.571793	2532.121792	17.709082	-0.047631	2.790458
245.719568	2524.108981	17.714087	-0.047653	2.786415
245.560710	2516.180773	17.719091	-0.047619	2.782392
245.382914	2508.206631	17.724096	-0.047580	2.778339
245.589885	2500.189736	17.729101	-0.047614	2.774280
245.401878	2492.213812	17.734106	-0.047574	2.770213
245.398778	2484.237973	17.739111	-0.047568	2.766151
245.365905	2476.295673	17.744115	-0.047557	2.762098
245.135103	2468.316102	17.749120	-0.047509	2.758009
245.167162	2460.325048	17.754125	-0.047510	2.753923
245.155949	2452.279658	17.759130	-0.047502	2.749801
245.098976	2444.306435	17.764135	-0.047487	2.745706
245.041725	2436.375524	17.769139	-0.047471	2.741628
244.818126	2428.411178	17.774144	-0.047424	2.737516
244.927557	2420.417805	17.779149	-0.047439	2.733403
244.959558	2412.428629	17.784154	-0.047440	2.729281
244.769775	2404.473536	17.789159	-0.047400	2.725157
244.577113	2396.539970	17.794163	-0.047359	2.721038
244.655039	2388.550885	17.799168	-0.047368	2.716901
244.682100	2380.558348	17.804173	-0.047368	2.712752
244.756719	2372.563357	17.809178	-0.047377	2.708598
244.619021	2364.592753	17.814183	-0.047346	2.704438
244.462153	2356.657113	17.819187	-0.047312	2.700288
244.408801	2348.682554	17.824192	-0.047297	2.696118
244.589736	2340.679143	17.829197	-0.047325	2.691941
244.444444	2332.722482	17.834202	-0.047293	2.687762
244.252125	2324.773240	17.839207	-0.047252	2.683577
244.295199	2316.816439	17.844211	-0.047255	2.679396
244.255980	2308.823317	17.849216	-0.047243	2.675184
244.036812	2300.835581	17.854221	-0.047197	2.670958
243.865550	2292.866031	17.859226	-0.047160	2.666737
243.840288	2284.889715	17.864231	-0.047150	2.662515
243.792924	2276.925804	17.869235	-0.047136	2.658291
243.682240	2268.954070	17.874240	-0.047110	2.654053
243.802551	2260.951130	17.879245	-0.047127	2.649806
243.627247	2252.998505	17.884250	-0.047090	2.645560
243.535200	2245.046225	17.889255	-0.047067	2.641313
243.592755	2237.076492	17.894259	-0.047073	2.637059
243.466927	2229.082613	17.899264	-0.047045	2.632773
243.444121	2221.085669	17.904269	-0.047035	2.628486
243.422227	2213.127820	17.909274	-0.047026	2.624212
243.278009	2205.178585	17.914279	-0.046994	2.619929
243.193111	2197.234820	17.919283	-0.046973	2.615645
242.942746	2189.252875	17.924288	-0.046921	2.611322
243.133998	2181.258751	17.929293	-0.046952	2.607015
243.103244	2173.294596	17.934298	-0.046941	2.602702
242.760814	2165.366553	17.939303	-0.046872	2.598381
242.851028	2157.347232	17.944307	-0.046884	2.594032
242.981655	2149.181153	17.949312	-0.046903	2.589598
242.829427	2141.267498	17.954317	-0.046869	2.585276
242.797627	2133.355253	17.959322	-0.046858	2.580955
242.694318	2125.394764	17.964327	-0.046834	2.576596
242.756851	2117.439539	17.969331	-0.046841	2.572243
242.434428	2109.506283	17.974336	-0.046776	2.567869
242.412428	2101.541282	17.979341	-0.046766	2.563490
242.542233	2093.580406	17.984346	-0.046785	2.559117
242.295429	2085.644088	17.989351	-0.046734	2.554723
242.400826	2077.628211	17.994355	-0.046749	2.550303
242.240497	2069.656131	17.999360	-0.046714	2.545880
242.077659	2061.727294	18.004365	-0.046678	2.541474
242.187660	2053.773169	18.009370	-0.046694	2.537065
242.083214	2045.785762	18.014375	-0.046669	2.532615
242.075417	2037.819457	18.019379	-0.046663	2.528175
241.991251	2029.846150	18.024384	-0.046642	2.523719
242.122073	2021.886567	18.029389	-0.046661	2.519277
242.137506	2013.937876	18.034394	-0.046659	2.514826
241.803576	2005.953788	18.039399	-0.046592	2.510321
241.679499	1997.991150	18.044403	-0.046563	2.505836
241.679217	1990.026100	18.049408	-0.046558	2.501350
241.573032	1982.079010	18.054413	-0.046533	2.496859
241.428209	1974.115390	18.059418	-0.046501	2.492347
241.354011	1966.130991	18.064423	-0.046482	2.487820
241.501415	1958.149284	18.069427	-0.046505	2.483303
241.295793	1950.228534	18.074432	-0.046461	2.478787
241.274174	1942.266706	18.079437	-0.046452	2.474252
241.438467	1934.257881	18.084442	-0.046478	2.469696
241.164466	1926.299987	18.089447	-0.046421	2.465128
241.284041	1918.365128	18.094451	-0.046439	2.460594
241.241087	1910.398582	18.099456	-0.046425	2.456021
241.120383	1902.430182	18.104461	-0.046398	2.451433
241.033307	1894.479954	18.109466	-0.046377	2.446849
240.723219	1886.547935	18.114471	-0.046314	2.442251
240.954433	1878.573508	18.119475	-0.046352	2.437660
240.864951	1870.562091	18.124480	-0.046330	2.433014
240.709359	1862.576337	18.129485	-0.046296	2.428370
240.929912	1854.601452	18.134490	-0.046332	2.423752
240.437547	1846.696086	18.139495	-0.046235	2.419110
240.465634	1838.739805	18.144499	-0.046235	2.414470
240.448302	1830.750916	18.149504	-0.046227	2.409799
240.540929	1822.783177	18.154509	-0.046239	2.405139
240.540475	1814.852470	18.159514	-0.046234	2.400485
240.164235	1806.935915	18.164519	-0.046159	2.395801
240.271632	1798.947381	18.169523	-0.046173	2.391103
240.295350	1790.966607	18.174528	-0.046173	2.386394
240.214203	1783.029013	18.179533	-0.046153	2.381693
240.223049	1775.075890	18.184538	-0.046149	2.376980
240.215640	1767.088704	18.189543	-0.046143	2.372236
240.011531	1759.162481	18.194547	-0.046099	2.367504
239.708888	1751.236695	18.199552	-0.046038	2.362754
239.708891	1743.272488	18.204557	-0.046033	2.357996
239.885132	1735.293049	18.209562	-0.046061	2.353234
239.679842	1727.322355	18.214567	-0.046017	2.348436
239.818084	1719.346050	18.219571	-0.046038	2.343653
239.657285	1711.425868	18.224576	-0.046003	2.338870
239.461950	1703.477830	18.229581	-0.045961	2.334057
239.518569	1695.505672	18.234586	-0.045967	2.329240
239.273080	1687.568106	18.239591	-0.045916	2.324409
239.041425	1679.659948	18.244595	-0.045868	2.319588
238.977925	1671.695497	18.249600	-0.045851	2.314735
239.157860	1663.678506	18.254605	-0.045879	2.309861
239.222187	1655.727271	18.259610	-0.045886	2.305007
239.058169	1647.791388	18.264615	-0.045850	2.300133
238.979533	1639.862247	18.269619	-0.045831	2.295260
238.819873	1631.901273	18.274624	-0.045796	2.290350
238.779714	1623.944584	18.279629	-0.045783	2.285443
238.819001	1616.021836	18.284634	-0.045786	2.280552
238.783780	1608.061572	18.289639	-0.045774	2.275622
238.809663	1600.031216	18.294643	-0.045773	2.270642
238.647543	1592.069507	18.299648	-0.045738	2.265678
238.405404	1584.170203	18.304653	-0.045688	2.260735
238.422520	1576.234419	18.309658	-0.045686	2.255781
238.223992	1568.277954	18.314663	-0.045644	2.250784
238.348272	1560.308588	18.319667	-0.045662	2.245796
238.151808	1552.391047	18.324672	-0.045620	2.240802
238.000778	1544.464408	18.329677	-0.045587	2.235795
238.148300	1536.478888	18.334682	-0.045610	2.230765
238.004472	1528.523152	18.339687	-0.045578	2.225717
237.871213	1520.616273	18.344691	-0.045548	2.220690
237.887260	1512.656667	18.349696	-0.045546	2.215631
237.891786	1504.687958	18.354701	-0.045541	2.210553
237.847753	1496.752663	18.359706	-0.045528	2.205481
237.677369	1488.831742	18.364711	-0.045491	2.200395
237.815851	1480.884258	18.369715	-0.045512	2.195308
237.727717	1472.899299	18.374720	-0.045490	2.190165
237.652407	1464.955517	18.379725	-0.045471	2.185037
237.509245	1457.048949	18.384730	-0.045440	2.179915
237.465677	1449.093259	18.389735	-0.045426	2.174758
237.447370	1441.150948	18.394739	-0.045418	2.169600
237.167270	1433.229019	18.399744	-0.045361	2.164418
237.010314	1425.311355	18.404749	-0.045326	2.159238
237.050823	1417.353659	18.409754	-0.045329	2.154038
236.983292	1409.395582	18.414759	-0.045311	2.148816
237.102723	1401.434446	18.419763	-0.045328	2.143595
237.039615	1393.507585	18.424768	-0.045311	2.138368
236.820357	1385.597946	18.429773	-0.045265	2.133124
237.016970	1377.628937	18.434778	-0.045297	2.127868
236.762685	1369.719312	18.439783	-0.045245	2.122595
236.800388	1361.799939	18.444787	-0.045246	2.117330
236.525952	1353.831790	18.449792	-0.045190	2.111989
236.589752	1345.851527	18.454797	-0.045197	2.106660
236.607130	1337.916003	18.459802	-0.045195	2.101342
236.505406	1329.996409	18.464807	-0.045171	2.096010
236.434371	1322.066432	18.469811	-0.045153	2.090661
236.443022	1314.116611	18.474816	-0.045149	2.085292
236.133589	1306.237097	18.479821	-0.045087	2.079925
236.072769	1298.330051	18.484826	-0.045070	2.074551
236.212923	1290.316478	18.489831	-0.045091	2.069110
236.146522	1282.417458	18.494835	-0.045074	2.063712
235.983931	1274.515126	18.499840	-0.045038	2.058288
235.877846	1266.576845	18.504845	-0.045014	2.052831
235.848025	1258.638148	18.509850	-0.045003	2.047366
235.717511	1250.718224	18.514855	-0.044973	2.041890
235.917266	1242.786944	18.519859	-0.045006	2.036425
235.765288	1234.838988	18.524864	-0.044972	2.030897
235.373504	1226.939972	18.529869	-0.044894	2.025364
235.522380	1219.001740	18.534874	-0.044917	2.019844
235.536725	1211.071691	18.539879	-0.044914	2.014300
235.434392	1203.139314	18.544883	-0.044890	2.008728
235.246609	1195.234103	18.549888	-0.044850	2.003150
235.229622	1187.311151	18.554893	-0.044842	1.997562
235.196189	1179.386560	18.559898	-0.044831	1.991955
234.998769	1171.457842	18.564903	-0.044789	1.986313
234.889951	1163.566673	18.569907	-0.044763	1.980690
234.800053	1155.651657	18.574912	-0.044742	1.975036
234.888352	1147.692905	18.579917	-0.044753	1.969354
234.623313	1139.816706	18.584922	-0.044699	1.963677
234.620246	1131.884022	18.589927	-0.044693	1.957970
234.846129	1123.920519	18.594931	-0.044730	1.952250
234.651343	1115.987798	18.599936	-0.044688	1.946489
234.344121	1108.105222	18.604941	-0.044626	1.940735
234.457312	1100.175392	18.609946	-0.044642	1.934976
234.420438	1092.230764	18.614951	-0.044630	1.929172
234.460166	1084.324264	18.619955	-0.044633	1.923387
234.404641	1076.424014	18.624960	-0.044617	1.917579
234.217676	1068.532224	18.629965	-0.044577	1.911744
234.014261	1060.632123	18.634970	-0.044534	1.905884
234.029834	1052.703128	18.639975	-0.044532	1.900009
234.085980	1044.798960	18.644979	-0.044538	1.894138
233.923736	1036.887571	18.649984	-0.044502	1.888219
233.832956	1028.985027	18.654989	-0.044480	1.882297
234.033086	1021.058990	18.659994	-0.044512	1.876371
233.734580	1013.156109	18.664999	-0.044452	1.870386
233.665864	1005.259792	18.670003	-0.044434	1.864414
233.537499	997.369526	18.675008	-0.044405	1.858420
233.499691	989.452198	18.680013	-0.044393	1.852397
233.427595	981.548496	18.685018	-0.044374	1.846361
233.176760	973.671180	18.690023	-0.044323	1.840303
233.327040	965.758422	18.695027	-0.044345	1.834246
233.277908	957.835506	18.700032	-0.044331	1.828138
233.175196	949.951350	18.705037	-0.044307	1.822032
233.237111	942.045602	18.710042	-0.044314	1.815909
233.150278	934.145704	18.715047	-0.044292	1.809752
233.007308	926.274012	18.720051	-0.044261	1.803589
233.021163	918.379203	18.725056	-0.044258	1.797405
232.833827	910.458608	18.730061	-0.044218	1.791156
232.693142	902.570403	18.735066	-0.044187	1.784916
232.475775	894.704251	18.740071	-0.044141	1.778662
232.837907	886.750566	18.745075	-0.044204	1.772388
232.560716	878.888560	18.750080	-0.044147	1.766085
232.225882	871.057969	18.755085	-0.044080	1.759778
232.314880	863.161476	18.760090	-0.044091	1.753448
232.398802	855.225714	18.765095	-0.044102	1.747063
232.345020	847.358857	18.770099	-0.044087	1.740693
232.157577	839.506409	18.775104	-0.044047	1.734294
232.164557	831.599821	18.780109	-0.044043	1.727852
232.077852	823.745745	18.785114	-0.044022	1.721417
231.915849	815.885075	18.790119	-0.043986	1.714943
231.999266	807.966430	18.795123	-0.043997	1.708428
231.861543	800.092533	18.800128	-0.043966	1.701896
231.811822	792.233001	18.805133	-0.043952	1.695362
231.689888	784.369374	18.810138	-0.043924	1.688791
231.637742	776.491508	18.815143	-0.043909	1.682191
231.551385	768.650152	18.820147	-0.043888	1.675591
231.466508	760.760255	18.825152	-0.043867	1.668924
231.501563	752.879017	18.830157	-0.043869	1.662254
231.543027	745.022802	18.835162	-0.043872	1.655579
231.332363	737.165279	18.840167	-0.043827	1.648842
231.110931	729.345556	18.845171	-0.043781	1.642108
231.061623	721.487925	18.850176	-0.043767	1.635337
231.102473	713.545172	18.855181	-0.043769	1.628476
231.084271	705.700123	18.860186	-0.043761	1.621664
230.989175	697.855443	18.865191	-0.043738	1.614812
230.954158	689.994253	18.870195	-0.043727	1.607925
230.725043	682.176225	18.875200	-0.043679	1.601019
230.722435	674.329449	18.880205	-0.043673	1.594090
230.827104	666.446611	18.885210	-0.043688	1.587114
230.552933	658.634917	18.890215	-0.043632	1.580116
230.466221	650.812525	18.895219	-0.043611	1.573104
230.329787	642.967199	18.900224	-0.043580	1.566033
230.053024	635.177285	18.905229	-0.043524	1.558959
229.977824	627.336781	18.910234	-0.043505	1.551837
229.961671	619.460156	18.915239	-0.043497	1.544658
229.958438	611.634662	18.920243	-0.043491	1.537494
229.802056	603.807424	18.925248	-0.043457	1.530272
229.687111	595.982859	18.930253	-0.043430	1.523024
229.613760	588.175398	18.935258	-0.043412	1.515764
229.448146	580.343587	18.940263	-0.043376	1.508432
229.720137	572.477936	18.945267	-0.043421	1.501099
229.461196	564.708218	18.950272	-0.043368	1.493739
229.163229	556.906086	18.955277	-0.043308	1.486306
229.180146	549.102190	18.960282	-0.043306	1.478883
229.165807	541.246257	18.965287	-0.043298	1.471367
228.941291	533.446545	18.970291	-0.043251	1.463834
228.921111	525.635069	18.975296	-0.043243	1.456283
228.783040	517.838364	18.980301	-0.043212	1.448688
228.861906	510.029843	18.985306	-0.043222	1.441077
228.694981	502.250687	18.990311	-0.043185	1.433414
228.638812	494.444634	18.995315	-0.043170	1.425701
228.653928	486.661159	19.000320	-0.043168	1.417981
228.519083	478.878263	19.005325	-0.043138	1.410193
228.350393	471.124150	19.010330	-0.043101	1.402386
228.167779	463.358992	19.015335	-0.043062	1.394522
228.240290	455.547095	19.020339	-0.043071	1.386609
228.186409	447.768682	19.025344	-0.043056	1.378663
228.046949	440.009245	19.030349	-0.043025	1.370675
228.087097	432.244685	19.035354	-0.043027	1.362667
227.725326	424.520625	19.040359	-0.042955	1.354583
227.855692	416.728731	19.045363	-0.042974	1.346466
227.907218	408.969275	19.050368	-0.042979	1.338320
227.666593	401.236385	19.055373	-0.042929	1.330100
227.562197	393.503884	19.060378	-0.042905	1.321854
227.454788	385.741654	19.065383	-0.042880	1.313524
227.383610	377.912331	19.070387	-0.042862	1.305074
227.103608	370.224319	19.075392	-0.042804	1.296685
226.968418	362.502585	19.080397	-0.042774	1.288231
227.143499	354.757170	19.085402	-0.042802	1.279753
226.901266	347.072018	19.090407	-0.042752	1.271206
226.717207	339.390151	19.095411	-0.042713	1.262617
226.869604	331.658658	19.100416	-0.042736	1.253977
226.928468	323.935983	19.105421	-0.042742	1.245269
226.738176	316.283506	19.110426	-0.042702	1.236531
226.522631	308.593194	19.115431	-0.042657	1.227683
226.548655	300.904256	19.120435	-0.042657	1.218819
226.385742	293.243926	19.125440	-0.042621	1.209887
225.997784	285.621088	19.130445	-0.042544	1.200887
226.117150	277.940700	19.135450	-0.042562	1.191853
225.945093	270.280307	19.140455	-0.042525	1.182715
225.985308	262.623871	19.145459	-0.042527	1.173554
225.899005	254.976707	19.150464	-0.042506	1.164306
225.831628	247.348887	19.155469	-0.042489	1.155011
225.570353	239.707215	19.160474	-0.042435	1.145583
225.513122	232.084949	19.165479	-0.042420	1.136144
225.233450	224.504872	19.170483	-0.042363	1.126631
225.045449	216.923807	19.175488	-0.042323	1.117055
225.113208	209.290878	19.180493	-0.042331	1.107387
225.243582	201.680135	19.185498	-0.042350	1.097675
224.836581	194.146389	19.190503	-0.042269	1.087857
224.780499	186.585058	19.195507	-0.042254	1.077992
224.655029	179.020218	19.200512	-0.042226	1.068016
224.589745	171.468045	19.205517	-0.042209	1.057976
224.539824	163.927935	19.210522	-0.042195	1.047860
224.285429	156.423757	19.215527	-0.042143	1.037646
224.239299	148.900735	19.220531	-0.042129	1.027354
224.017531	141.423832	19.225536	-0.042083	1.016980
223.954782	133.918388	19.230541	-0.042067	1.006497
223.866421	126.455092	19.235546	-0.042045	0.995957
223.644644	118.965880	19.240551	-0.041999	0.985234
223.598959	111.506421	19.245555	-0.041986	0.974481
223.471845	104.067031	19.250560	-0.041957	0.963616
223.168033	96.684989	19.255565	-0.041896	0.952666
222.928304	89.298285	19.260570	-0.041847	0.941598
222.701241	81.915876	19.265575	-0.041800	0.930409
222.673742	74.530073	19.270579	-0.041790	0.919132
222.467689	67.177913	19.275584	-0.041747	0.907718
221.936768	60.131270	19.280589	-0.041643	0.896550