Tue Mar 23 11:17:21 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.688512	-0.101822	0.000000	-0.000005	0.722704

0.770103	-0.118327	0.005005	-0.000020	0.722700
0.551413	-0.078076	0.010010	0.000020	0.722703
0.683799	-0.105730	0.015014	-0.000005	0.722695
0.941972	-0.148223	0.020019	-0.000053	0.722702
0.531200	-0.078350	0.025024	0.000024	0.722696
0.650938	-0.098385	0.030029	0.000001	0.722699
0.544103	-0.080790	0.035034	0.000021	0.722696
0.518333	-0.079494	0.040038	0.000026	0.722690
0.518240	-0.073546	0.045043	0.000026	0.722702
0.494931	-0.073642	0.050048	0.000030	0.722693
0.506033	-0.072549	0.055053	0.000028	0.722700
0.457877	-0.063173	0.060058	0.000036	0.722702
0.466816	-0.069090	0.065062	0.000035	0.722693
0.578850	-0.083142	0.070067	0.000014	0.722705
0.598516	-0.093632	0.075072	0.000010	0.722692
0.723074	-0.227457	0.080077	-0.000013	0.722473
0.630153	-0.259511	0.085082	0.000004	0.722377
0.395804	-0.222393	0.090086	0.000047	0.722368
0.575516	-0.248934	0.095091	0.000014	0.722379
0.722218	-0.279771	0.100096	-0.000014	0.722370
0.536437	-0.244663	0.105101	0.000021	0.722375
0.592423	-0.284584	0.110106	0.000010	0.722316
0.518205	-0.392616	0.115110	0.000024	0.722078
0.675984	-0.416685	0.120115	-0.000005	0.722086
0.528569	-0.396987	0.125120	0.000022	0.722073
0.629328	-0.413646	0.130125	0.000003	0.722076
0.590607	-0.443367	0.135130	0.000010	0.722004
0.394274	-0.542510	0.140134	0.000047	0.721741
0.481802	-0.551772	0.145139	0.000030	0.721754
0.440426	-0.548885	0.150144	0.000038	0.721745
0.455578	-0.551535	0.155149	0.000035	0.721746
0.414998	-0.679906	0.160154	0.000042	0.721479
0.480123	-0.713242	0.165158	0.000030	0.721437
0.654956	-0.739797	0.170163	-0.000002	0.721446
0.549007	-0.749143	0.175168	0.000017	0.721391
0.616451	-0.893864	0.180173	0.000005	0.721130
0.423295	-0.857563	0.185178	0.000040	0.721134
0.448251	-0.867235	0.190182	0.000036	0.721124
0.482475	-0.960504	0.195187	0.000029	0.720952
0.440131	-0.989047	0.200192	0.000037	0.720881
0.578691	-1.011448	0.205197	0.000011	0.720886
0.561461	-1.120307	0.210202	0.000014	0.720666
0.481012	-1.168926	0.215206	0.000029	0.720542
0.232237	-1.120265	0.220211	0.000075	0.720551
0.121978	-1.219283	0.225216	0.000096	0.720318
0.187380	-1.276685	0.230221	0.000084	0.720228
0.069459	-1.255246	0.235226	0.000105	0.720229
0.038267	-1.387061	0.240230	0.000111	0.719958
0.222781	-1.444778	0.245235	0.000077	0.719910
0.381364	-1.497243	0.250240	0.000047	0.719862
0.352149	-1.621346	0.255245	0.000053	0.719607
0.262390	-1.605396	0.260250	0.000069	0.719608
0.364340	-1.736859	0.265254	0.000050	0.719384
0.407597	-1.798688	0.270259	0.000042	0.719278
0.206474	-1.813986	0.275264	0.000079	0.719177
0.075829	-1.897796	0.280269	0.000104	0.718966
0.361800	-1.948156	0.285274	0.000050	0.718968
-0.078357	-2.032606	0.290278	0.000132	0.718646
-0.342373	-1.981316	0.295283	0.000181	0.718655
-0.595135	-2.033182	0.300288	0.000228	0.718464
-0.536659	-2.096149	0.305293	0.000217	0.718360
-0.602018	-2.126744	0.310298	0.000229	0.718277
-0.374183	-2.298110	0.315302	0.000187	0.718019
-0.573629	-2.261125	0.320307	0.000224	0.718022
-2.430994	-2.090329	0.325312	0.000569	0.717706
-2.415418	-2.091319	0.330317	0.000566	0.717710
-2.346269	-2.120681	0.335322	0.000554	0.717676
-2.969428	-2.161261	0.340326	0.000669	0.717377
-2.818682	-2.181707	0.345331	0.000641	0.717390
-3.535784	-2.065162	0.350336	0.000775	0.717368
-3.938207	-2.134449	0.355341	0.000849	0.717089
-3.790489	-2.161774	0.360346	0.000822	0.717088
-4.331621	-2.067449	0.365350	0.000922	0.717084
-4.121214	-2.200747	0.370355	0.000883	0.716894
-5.497103	-2.026125	0.375360	0.001139	0.716755
-4.935609	-2.124460	0.380365	0.001035	0.716759
-4.580562	-2.186423	0.385370	0.000968	0.716761
-5.699753	-2.108226	0.390374	0.001177	0.716522
-6.128611	-2.063801	0.395379	0.001256	0.716459
-5.714775	-2.142384	0.400384	0.001179	0.716449
-5.991836	-2.091536	0.405389	0.001231	0.716452
-5.767668	-2.189258	0.410394	0.001189	0.716338
-6.974843	-2.078294	0.415398	0.001413	0.716132
-6.804932	-2.102956	0.420403	0.001382	0.716144
-7.046915	-2.062924	0.425408	0.001427	0.716138
-6.771346	-2.111878	0.430413	0.001375	0.716138
-6.770146	-2.180457	0.435418	0.001375	0.716003
-8.069994	-2.009702	0.440422	0.001617	0.715883
-7.092941	-2.179539	0.445427	0.001435	0.715891
-7.489379	-2.112508	0.450432	0.001508	0.715884
-8.029861	-2.016711	0.455437	0.001609	0.715884
-7.705326	-2.166156	0.460442	0.001548	0.715702
-8.753189	-2.058078	0.465446	0.001743	0.715547
-8.584654	-2.083484	0.470451	0.001712	0.715556
-8.858049	-2.038601	0.475456	0.001763	0.715549
-8.579198	-2.086922	0.480461	0.001711	0.715552
-8.318768	-2.132434	0.485466	0.001662	0.715554
-9.517253	-2.072494	0.490470	0.001885	0.715249
-9.584494	-2.063815	0.495475	0.001898	0.715243
-9.382380	-2.104252	0.500480	0.001860	0.715234
-9.507676	-2.080867	0.505485	0.001883	0.715237
-9.545800	-2.071591	0.510490	0.001890	0.715242
-9.595105	-2.068821	0.515494	0.001899	0.715230
-9.644083	-2.181776	0.520499	0.001908	0.714989
-10.900653	-1.998218	0.525504	0.002142	0.714909
-10.518840	-2.063270	0.530509	0.002071	0.714915
-10.074983	-2.142204	0.535514	0.001988	0.714916
-10.717169	-2.030762	0.540518	0.002107	0.714910
-10.341368	-2.094153	0.545523	0.002037	0.714917
-10.317694	-2.151203	0.550528	0.002033	0.714813
-11.822565	-1.983539	0.555533	0.002313	0.714614
-11.325206	-2.073261	0.560538	0.002220	0.714612
-11.497557	-2.045346	0.565542	0.002252	0.714606
-11.734576	-1.997659	0.570547	0.002296	0.714617
-11.697923	-2.007561	0.575552	0.002289	0.714611
-11.482585	-2.045989	0.580557	0.002249	0.714611
-11.309876	-2.113017	0.585562	0.002217	0.714539
-12.680496	-2.002061	0.590566	0.002472	0.714275
-12.138013	-2.094637	0.595571	0.002371	0.714283
-12.394480	-2.051030	0.600576	0.002418	0.714279
-12.323299	-2.063113	0.605581	0.002405	0.714281
-12.471474	-2.035456	0.610586	0.002432	0.714283
-12.697427	-2.001015	0.615590	0.002474	0.714272
-12.195156	-2.110469	0.620595	0.002381	0.714232
-13.411833	-2.027968	0.625600	0.002607	0.713966
-13.598002	-1.993032	0.630605	0.002642	0.713970
-13.456630	-2.017934	0.635610	0.002615	0.713970
-13.322680	-2.044379	0.640614	0.002590	0.713966
-13.262097	-2.049431	0.645619	0.002579	0.713977
-13.505069	-2.009561	0.650624	0.002624	0.713971
-13.353460	-2.035461	0.655629	0.002596	0.713973
-13.283201	-2.151570	0.660634	0.002582	0.713767
-14.632753	-1.970706	0.665638	0.002833	0.713649
-13.770779	-2.118437	0.670643	0.002673	0.713661
-14.138833	-2.057381	0.675648	0.002741	0.713652
-14.482256	-1.993963	0.680653	0.002805	0.713657
-13.797412	-2.117323	0.685658	0.002678	0.713654
-14.197043	-2.049308	0.690662	0.002752	0.713648
-14.638540	-2.093274	0.695667	0.002834	0.713405
-15.175046	-2.021039	0.700672	0.002934	0.713358
-14.986520	-2.052693	0.705677	0.002898	0.713362
-15.196074	-2.015986	0.710682	0.002937	0.713361
-15.137567	-2.028794	0.715686	0.002926	0.713357
-14.690950	-2.104738	0.720691	0.002843	0.713364
-14.923537	-2.067536	0.725696	0.002886	0.713356
-15.764338	-2.077215	0.730701	0.003043	0.713039
-15.945064	-2.047288	0.735706	0.003076	0.713035
-16.272988	-1.992982	0.740710	0.003137	0.713027
-15.745867	-2.080996	0.745715	0.003039	0.713039
-15.960582	-2.047994	0.750720	0.003079	0.713028
-16.106154	-2.021546	0.755725	0.003106	0.713030
-16.036473	-2.032502	0.760730	0.003093	0.713033
-16.418883	-2.074533	0.765734	0.003164	0.712814
-17.175907	-1.987445	0.770739	0.003305	0.712719
-17.213017	-1.983532	0.775744	0.003311	0.712714
-17.031433	-2.015208	0.780749	0.003277	0.712715
-16.723007	-2.068304	0.785754	0.003220	0.712719
-17.115966	-2.003310	0.790758	0.003293	0.712709
-16.942482	-2.029075	0.795763	0.003261	0.712720
-17.043285	-2.025651	0.800768	0.003279	0.712691
-17.413613	-2.111146	0.805773	0.003348	0.712390
-17.519855	-2.090137	0.810778	0.003368	0.712394
-18.238064	-1.965121	0.815782	0.003501	0.712388
-17.712957	-2.054078	0.820787	0.003403	0.712398
-17.697392	-2.064209	0.825792	0.003400	0.712383
-17.932896	-2.019037	0.830797	0.003444	0.712390
-17.760287	-2.064940	0.835802	0.003412	0.712360
-18.767374	-2.021689	0.840806	0.003599	0.712089
-18.525394	-2.058723	0.845811	0.003554	0.712101
-18.801929	-2.014033	0.850816	0.003605	0.712092
-18.514810	-2.063141	0.855821	0.003552	0.712097
-18.655312	-2.037517	0.860826	0.003578	0.712098
-18.951474	-1.989017	0.865830	0.003633	0.712090
-18.673624	-2.030914	0.870835	0.003581	0.712105
-19.437999	-2.051514	0.875840	0.003723	0.711793
-20.075505	-1.950731	0.880845	0.003842	0.711767
-19.694068	-2.017545	0.885850	0.003771	0.711770
-19.640577	-2.032626	0.890854	0.003761	0.711759
-20.010810	-1.960908	0.895859	0.003830	0.711771
-20.077247	-1.953840	0.900864	0.003842	0.711761
-19.469669	-2.060121	0.905869	0.003729	0.711766
-19.525597	-2.087876	0.910874	0.003739	0.711691
-20.828534	-1.974837	0.915878	0.003981	0.711453
-20.327565	-2.061893	0.920883	0.003888	0.711458
-20.656580	-2.004717	0.925888	0.003949	0.711455
-20.862435	-1.966862	0.930893	0.003987	0.711458
-20.485745	-2.033067	0.935898	0.003917	0.711460
-20.853735	-1.971803	0.940902	0.003985	0.711451
-20.564257	-2.018364	0.945907	0.003931	0.711462
-20.883913	-2.098412	0.950912	0.003991	0.711189
-21.606153	-1.992174	0.955917	0.004125	0.711144
-21.522936	-2.005586	0.960922	0.004110	0.711147
-21.666109	-1.985234	0.965926	0.004136	0.711137
-21.508083	-2.008612	0.970931	0.004107	0.711147
-21.386852	-2.035092	0.975936	0.004084	0.711137
-21.688115	-1.980278	0.980941	0.004140	0.711140
-21.535022	-2.081126	0.985946	0.004111	0.710993
-22.356164	-1.995446	0.990950	0.004264	0.710872
-22.078490	-2.041395	0.995955	0.004212	0.710879
-22.514314	-1.967765	1.000960	0.004293	0.710872
-22.361690	-1.993662	1.005965	0.004265	0.710874
-21.644930	-2.118780	1.010970	0.004131	0.710880
-22.425740	-1.985444	1.015974	0.004276	0.710869
-22.768073	-2.088285	1.020979	0.004340	0.710541
-22.796407	-2.087138	1.025984	0.004345	0.710534
-23.547782	-1.952165	1.030989	0.004485	0.710536
-22.984852	-2.050230	1.035994	0.004380	0.710541
-23.109972	-2.033127	1.040998	0.004403	0.710531
-23.256133	-2.003017	1.046003	0.004430	0.710539
-23.498922	-1.968581	1.051008	0.004475	0.710522
-23.872754	-2.052098	1.056013	0.004545	0.710222
-23.883439	-2.050384	1.061018	0.004547	0.710222
-24.644792	-1.917379	1.066022	0.004688	0.710217
-23.951720	-2.036371	1.071027	0.004559	0.710226
-23.748947	-2.074837	1.076032	0.004521	0.710222
-24.350305	-1.967762	1.081037	0.004633	0.710222
-24.024734	-2.022212	1.086042	0.004573	0.710229
-24.471904	-2.094002	1.091046	0.004656	0.709926
-24.997396	-2.011565	1.096051	0.004753	0.709904
-25.333477	-1.956712	1.101056	0.004816	0.709894
-24.829680	-2.047097	1.106061	0.004722	0.709893
-24.650591	-2.077128	1.111066	0.004689	0.709897
-25.330160	-1.957910	1.116070	0.004815	0.709894
-24.905373	-2.029963	1.121075	0.004736	0.709901
-25.277231	-2.086188	1.126080	0.004805	0.709657
-26.309383	-1.930867	1.131085	0.004997	0.709600
-25.883503	-2.004561	1.136090	0.004917	0.709604
-25.810175	-2.021834	1.141094	0.004904	0.709596
-25.455868	-2.080045	1.146099	0.004838	0.709606
-25.855956	-2.013393	1.151104	0.004912	0.709597
-25.809831	-2.022581	1.156109	0.004903	0.709595
-25.919923	-2.135649	1.161114	0.004924	0.709330
-27.112679	-1.956215	1.166118	0.005146	0.709264
-26.769699	-2.013425	1.171123	0.005082	0.709272
-26.284722	-2.103150	1.176128	0.004991	0.709266
-26.838160	-2.002463	1.181133	0.005094	0.709270
-26.742744	-2.018718	1.186138	0.005076	0.709272
-26.736368	-2.021525	1.191142	0.005075	0.709269
-27.092171	-2.094136	1.196147	0.005141	0.708996
-27.935271	-1.963502	1.201152	0.005298	0.708957
-27.827911	-1.980912	1.206157	0.005278	0.708961
-27.384802	-2.059553	1.211162	0.005195	0.708962
-27.814222	-1.987277	1.216166	0.005275	0.708954
-27.523638	-2.034608	1.221171	0.005221	0.708963
-27.440205	-2.053328	1.226176	0.005205	0.708955
-27.956476	-2.083917	1.231181	0.005301	0.708710
-28.706760	-1.980992	1.236186	0.005441	0.708649
-28.836530	-1.962147	1.241190	0.005465	0.708640
-28.252473	-2.062556	1.246195	0.005356	0.708648
-28.753698	-1.975766	1.251200	0.005449	0.708643
-28.748062	-1.977428	1.256205	0.005448	0.708642
-28.187217	-2.074869	1.261210	0.005344	0.708647
-28.633174	-2.072287	1.266214	0.005426	0.708493
-29.513641	-1.982250	1.271219	0.005590	0.708360
-29.187689	-2.044417	1.276224	0.005529	0.708352
-29.530185	-1.982173	1.281229	0.005593	0.708354
-29.395687	-2.005005	1.286234	0.005568	0.708357
-29.258155	-2.032156	1.291238	0.005542	0.708352
-29.271289	-2.026734	1.296243	0.005545	0.708358
-29.535676	-2.081777	1.301248	0.005594	0.708153
-30.846235	-1.918834	1.306253	0.005837	0.708012
-29.864046	-2.090939	1.311258	0.005655	0.708018
-30.341489	-2.009082	1.316262	0.005743	0.708012
-30.676475	-1.945800	1.321267	0.005806	0.708019
-30.252964	-2.024029	1.326272	0.005727	0.708014
-30.049420	-2.059012	1.331277	0.005689	0.708017
-30.116151	-2.118720	1.336282	0.005701	0.707874
-31.729640	-1.919422	1.341286	0.006001	0.707697
-30.761004	-2.086471	1.346291	0.005821	0.707708
-31.115542	-2.027408	1.351296	0.005887	0.707700
-31.443561	-1.968598	1.356301	0.005948	0.707701
-30.907579	-2.061151	1.361306	0.005848	0.707707
-31.452960	-1.969129	1.366310	0.005949	0.707697
-31.329468	-2.039988	1.371315	0.005926	0.707599
-32.000573	-2.031687	1.376320	0.006051	0.707376
-31.935426	-2.043330	1.381325	0.006039	0.707376
-32.295492	-1.975813	1.386330	0.006106	0.707383
-32.086655	-2.018935	1.391334	0.006067	0.707372
-31.745347	-2.072834	1.396339	0.006003	0.707386
-32.037420	-2.024666	1.401344	0.006057	0.707378
-32.339512	-2.019386	1.406349	0.006113	0.707281
-32.807968	-2.032220	1.411354	0.006200	0.707088
-32.816946	-2.034152	1.416358	0.006202	0.707081
-33.224387	-1.956132	1.421363	0.006278	0.707092
-33.243981	-1.957571	1.426368	0.006281	0.707082
-32.803748	-2.034895	1.431373	0.006199	0.707085
-32.713223	-2.049740	1.436378	0.006182	0.707088
-33.064238	-2.009293	1.441382	0.006247	0.707043
-33.672927	-2.041933	1.446387	0.006361	0.706760
-33.731509	-2.033624	1.451392	0.006371	0.706756
-34.056983	-1.975613	1.456397	0.006432	0.706756
-33.608432	-2.052129	1.461402	0.006348	0.706763
-33.819271	-2.020609	1.466406	0.006387	0.706751
-34.020403	-1.980019	1.471411	0.006425	0.706761
-33.687406	-2.056725	1.476416	0.006363	0.706727
-34.411470	-2.065434	1.481421	0.006497	0.706450
-34.592923	-2.032663	1.486426	0.006531	0.706451
-35.028481	-1.958332	1.491430	0.006612	0.706445
-34.438623	-2.060968	1.496435	0.006502	0.706450
-34.253654	-2.097811	1.501440	0.006468	0.706442
-35.050817	-1.954569	1.506445	0.006616	0.706445
-34.819726	-2.017765	1.511450	0.006573	0.706401
-35.257910	-2.077316	1.516454	0.006654	0.706124
-35.339334	-2.058414	1.521459	0.006669	0.706133
-35.551569	-2.023028	1.526464	0.006709	0.706129
-35.479119	-2.036595	1.531469	0.006695	0.706128
-35.451571	-2.039249	1.536474	0.006690	0.706132
-35.849460	-1.971240	1.541478	0.006764	0.706127
-35.555871	-2.064969	1.546483	0.006709	0.706044
-36.349188	-2.012776	1.551488	0.006857	0.705864
-36.415277	-2.001264	1.556493	0.006869	0.705864
-36.324802	-2.014009	1.561498	0.006852	0.705871
-36.426474	-2.003448	1.566502	0.006871	0.705856
-36.285626	-2.020865	1.571507	0.006844	0.705872
-36.442347	-1.996691	1.576512	0.006873	0.705865
-36.418295	-2.079564	1.581517	0.006869	0.705707
-37.402549	-1.991585	1.586522	0.007052	0.705531
-37.402075	-1.997016	1.591526	0.007052	0.705520
-37.248019	-2.019196	1.596531	0.007023	0.705531
-37.369111	-1.999469	1.601536	0.007045	0.705528
-37.395655	-1.995082	1.606541	0.007050	0.705527
-37.286489	-2.013798	1.611546	0.007030	0.705529
-37.183750	-2.087163	1.616550	0.007010	0.705418
-38.224505	-2.001088	1.621555	0.007204	0.705218
-38.153877	-2.017005	1.626560	0.007191	0.705212
-38.488828	-1.956447	1.631565	0.007253	0.705214
-38.063744	-2.031006	1.636570	0.007174	0.705217
-38.401923	-1.975337	1.641574	0.007237	0.705207
-38.238752	-1.999765	1.646579	0.007206	0.705217
-38.132700	-2.045870	1.651584	0.007186	0.705163
-38.956090	-2.035689	1.656589	0.007339	0.704888
-38.916456	-2.039921	1.661594	0.007332	0.704894
-39.118515	-2.008627	1.666598	0.007369	0.704884
-38.976722	-2.031223	1.671603	0.007343	0.704890
-39.119983	-2.006225	1.676608	0.007370	0.704889
-39.054565	-2.019430	1.681613	0.007357	0.704886
-38.831336	-2.109727	1.686618	0.007316	0.704785
-40.329878	-1.940094	1.691622	0.007594	0.704588
-39.935403	-2.006530	1.696627	0.007521	0.704596
-39.828950	-2.026778	1.701632	0.007501	0.704594
-40.182959	-1.965493	1.706637	0.007567	0.704591
-39.936187	-2.005524	1.711642	0.007521	0.704599
-39.933678	-2.011155	1.716646	0.007520	0.704589
-40.093829	-2.000571	1.721651	0.007550	0.704553
-41.157782	-1.954694	1.726656	0.007748	0.704263
-41.043770	-1.975361	1.731661	0.007726	0.704263
-40.844612	-2.008224	1.736666	0.007689	0.704268
-40.901991	-2.002171	1.741670	0.007700	0.704260
-40.978237	-1.987337	1.746675	0.007714	0.704263
-41.043071	-1.976976	1.751680	0.007726	0.704260
-40.759776	-2.028165	1.756685	0.007673	0.704259
-41.001519	-2.086651	1.761690	0.007718	0.704055
-41.853173	-1.987763	1.766694	0.007876	0.703948
-41.416576	-2.061947	1.771699	0.007795	0.703956
-41.559061	-2.037897	1.776704	0.007821	0.703953
-41.833608	-1.989573	1.781709	0.007872	0.703952
-41.565319	-2.032749	1.786714	0.007822	0.703962
-41.860756	-1.984608	1.791718	0.007877	0.703953
-42.379660	-2.041477	1.796723	0.007974	0.703652
-42.370047	-2.049953	1.801728	0.007972	0.703638
-42.730754	-1.987815	1.806733	0.008039	0.703634
-42.622451	-2.003984	1.811738	0.008019	0.703641
-42.583633	-2.014688	1.816742	0.008011	0.703633
-42.413904	-2.040686	1.821747	0.007979	0.703642
-42.644624	-2.009569	1.826752	0.008022	0.703622
-43.644142	-1.969324	1.831757	0.008208	0.703344
-43.011472	-2.080400	1.836762	0.008090	0.703347
-43.406562	-2.013213	1.841766	0.008164	0.703341
-43.218151	-2.043702	1.846771	0.008129	0.703348
-43.118618	-2.063760	1.851776	0.008110	0.703343
-43.435472	-2.006963	1.856781	0.008169	0.703344
-43.365803	-2.093154	1.861786	0.008156	0.703195
-44.500320	-1.986957	1.866790	0.008367	0.703001
-43.893020	-2.092393	1.871795	0.008254	0.703007
-44.155588	-2.046856	1.876800	0.008303	0.703005
-44.544306	-1.977557	1.881805	0.008375	0.703005
-44.078093	-2.058769	1.886810	0.008288	0.703009
-44.447044	-1.996084	1.891814	0.008356	0.703003
-44.646397	-2.039070	1.896819	0.008393	0.702845
-45.299188	-1.998461	1.901824	0.008515	0.702692
-45.238870	-2.009364	1.906829	0.008503	0.702692
-45.347209	-1.985991	1.911834	0.008524	0.702700
-45.684317	-1.932223	1.916838	0.008586	0.702688
-45.031966	-2.043455	1.921843	0.008465	0.702698
-45.254105	-2.005665	1.926848	0.008506	0.702695
-45.596502	-1.946320	1.931853	0.008569	0.702692
-45.652452	-2.092071	1.936858	0.008580	0.702377
-46.072399	-2.022489	1.941862	0.008658	0.702367
-46.398843	-1.958923	1.946867	0.008719	0.702378
-46.236710	-1.991837	1.951872	0.008688	0.702370
-46.295577	-1.980566	1.956877	0.008699	0.702372
-46.019232	-2.024964	1.961882	0.008648	0.702382
-46.073533	-2.021531	1.966886	0.008658	0.702369
-46.588567	-2.057472	1.971891	0.008753	0.702111
-47.135623	-1.977417	1.976896	0.008855	0.702076
-47.440854	-1.922572	1.981901	0.008912	0.702077
-46.668315	-2.058789	1.986906	0.008768	0.702080
-47.238784	-1.960517	1.991910	0.008874	0.702074
-47.263671	-1.951446	1.996915	0.008878	0.702083
-46.887971	-2.061811	2.001920	0.008808	0.701996

-48.164179	-1.957192	2.011917	0.009046	0.701747
-47.824483	-2.017783	2.021914	0.008982	0.701748
-48.020471	-1.982794	2.031910	0.009019	0.701748
-48.000576	-1.987568	2.041907	0.009015	0.701746
-48.036521	-1.982424	2.051904	0.009021	0.701744
-47.935900	-1.998771	2.061901	0.009002	0.701748
-47.854824	-2.014452	2.071898	0.008987	0.701746
-47.784356	-2.027083	2.081894	0.008973	0.701746
-47.961142	-1.996869	2.091891	0.009006	0.701744
-47.727281	-1.994807	2.101888	0.008962	0.701833
-47.182771	-1.971687	2.111885	0.008861	0.702077
-46.778990	-2.042736	2.121882	0.008785	0.702079
-47.335954	-1.943510	2.131878	0.008889	0.702079
-47.128615	-1.983091	2.141875	0.008850	0.702074
-47.311559	-1.951278	2.151872	0.008884	0.702073
-47.183563	-1.931402	2.161869	0.008860	0.702160
-46.238636	-1.993673	2.171866	0.008683	0.702375
-46.285242	-1.985471	2.181862	0.008692	0.702375
-46.214804	-1.998946	2.191859	0.008679	0.702374
-46.528433	-1.944107	2.201856	0.008737	0.702372
-45.721777	-1.937929	2.211853	0.008586	0.702676
-45.281440	-2.006792	2.221850	0.008504	0.702696
-45.488561	-1.969820	2.231846	0.008542	0.702696
-45.396414	-1.988596	2.241843	0.008525	0.702692
-44.791343	-1.954491	2.251840	0.008412	0.702980
-44.700131	-1.960066	2.261837	0.008395	0.703002
-44.469540	-2.000080	2.271834	0.008352	0.703004
-44.641783	-1.936563	2.281830	0.008384	0.703071
-43.608093	-1.988805	2.291827	0.008191	0.703338
-43.833251	-1.950052	2.301824	0.008233	0.703336
-43.645314	-1.983118	2.311821	0.008197	0.703337
-43.350803	-1.962110	2.321818	0.008142	0.703486
-42.968643	-1.957405	2.331814	0.008071	0.703633
-42.966313	-1.957617	2.341811	0.008070	0.703634
-43.201964	-1.898255	2.351808	0.008114	0.703670
-41.934865	-1.985510	2.361805	0.007878	0.703950
-41.992163	-1.974473	2.371802	0.007888	0.703952
-42.125316	-1.948908	2.381798	0.007913	0.703956
-41.689429	-1.930480	2.391795	0.007831	0.704151
-41.330968	-1.941241	2.401792	0.007764	0.704258
-41.078817	-1.985014	2.411789	0.007717	0.704261
-41.135915	-1.948047	2.421786	0.007728	0.704315
-40.328003	-1.956876	2.431782	0.007577	0.704588
-40.036491	-2.009408	2.441779	0.007522	0.704588
-40.287299	-1.965313	2.451776	0.007569	0.704587
-39.894928	-1.964514	2.461773	0.007496	0.704730
-39.221986	-2.005292	2.471770	0.007370	0.704890
-39.293447	-1.992118	2.481766	0.007383	0.704891
-39.300000	-1.993305	2.491763	0.007384	0.704887
-38.759871	-1.959871	2.501760	0.007283	0.705149
-38.395481	-1.992290	2.511757	0.007215	0.705215
-38.455148	-1.981994	2.521754	0.007226	0.705214
-38.287164	-1.973774	2.531750	0.007195	0.705292
-37.664998	-1.968160	2.541747	0.007078	0.705527
-37.613002	-1.979552	2.551744	0.007069	0.705523
-37.534210	-1.993585	2.561741	0.007054	0.705523
-37.065690	-1.952699	2.571738	0.006966	0.705774
-36.750585	-1.963248	2.581734	0.006907	0.705866
-36.757250	-1.963254	2.591731	0.006908	0.705864
-36.735202	-1.922615	2.601728	0.006904	0.705954
-35.931093	-1.978766	2.611725	0.006754	0.706130
-35.892130	-1.985583	2.621722	0.006746	0.706131
-35.884831	-1.987262	2.631718	0.006745	0.706131
-35.500146	-1.904843	2.641715	0.006673	0.706435
-35.112118	-1.969128	2.651712	0.006601	0.706445
-35.089758	-1.972791	2.661709	0.006596	0.706446
-34.601998	-1.957948	2.671706	0.006505	0.706651
-34.199324	-1.977779	2.681702	0.006430	0.706756
-34.488774	-1.927466	2.691699	0.006484	0.706754
-34.288477	-1.908498	2.701696	0.006446	0.706864
-33.283192	-1.980528	2.711693	0.006259	0.707080
-33.666338	-1.910133	2.721690	0.006330	0.707084
-33.153247	-2.002341	2.731686	0.006234	0.707083
-32.724998	-1.939342	2.741683	0.006154	0.707363
-32.314339	-2.005195	2.751680	0.006077	0.707378
-32.401096	-1.990502	2.761677	0.006093	0.707377
-32.339914	-1.945171	2.771674	0.006082	0.707491
-31.359229	-2.015007	2.781670	0.005899	0.707702
-31.679190	-1.958327	2.791667	0.005958	0.707701
-31.674390	-1.960613	2.801664	0.005957	0.707699
-31.007074	-1.941762	2.811661	0.005832	0.707976
-30.662853	-1.983647	2.821658	0.005768	0.708015
-30.538813	-2.005545	2.831654	0.005745	0.708016
-30.895872	-1.880405	2.841651	0.005811	0.708140
-29.685838	-1.989834	2.851648	0.005586	0.708353
-29.935335	-1.945908	2.861645	0.005632	0.708353
-29.763504	-1.976127	2.871642	0.005600	0.708354
-28.944836	-1.996744	2.881638	0.005447	0.708605
-28.968428	-1.975132	2.891635	0.005451	0.708641
-28.899337	-1.988681	2.901632	0.005438	0.708639
-28.953258	-1.936620	2.911629	0.005448	0.708724
-27.870652	-2.013055	2.921626	0.005246	0.708958
-27.778370	-2.028239	2.931622	0.005229	0.708961
-28.052248	-1.980790	2.941619	0.005279	0.708959
-27.403189	-2.008853	2.951616	0.005158	0.709134
-27.303428	-1.961932	2.961613	0.005139	0.709264
-26.968061	-2.021327	2.971610	0.005077	0.709266
-27.089732	-1.995692	2.981606	0.005099	0.709274
-26.352216	-1.963625	2.991603	0.004962	0.709602
-26.188540	-1.993871	3.001600	0.004931	0.709600
-26.302133	-1.974244	3.011597	0.004952	0.709599
-26.033118	-1.953451	3.021594	0.004901	0.709737
-25.426851	-1.982067	3.031590	0.004788	0.709896
-25.539915	-1.961636	3.041587	0.004809	0.709897
-25.418209	-1.955719	3.051584	0.004786	0.709953
-24.671583	-1.955719	3.061581	0.004647	0.710219
-24.423690	-1.997334	3.071578	0.004601	0.710225
-24.717638	-1.944635	3.081574	0.004655	0.710226
-24.016878	-1.944738	3.091571	0.004524	0.710476
-23.881783	-1.938210	3.101568	0.004499	0.710537
-23.600849	-1.988447	3.111565	0.004446	0.710537
-23.547868	-1.942171	3.121562	0.004436	0.710649
-22.568990	-2.001606	3.131558	0.004254	0.710879
-22.742907	-1.970607	3.141555	0.004286	0.710880
-22.666920	-1.985385	3.151552	0.004272	0.710878
-22.359980	-1.962681	3.161549	0.004214	0.711033
-21.902171	-1.986845	3.171546	0.004129	0.711148
-22.228984	-1.929585	3.181542	0.004189	0.711146
-21.851373	-1.941565	3.191539	0.004119	0.711257
-21.187794	-1.957249	3.201536	0.003995	0.711462
-21.338397	-1.931189	3.211533	0.004023	0.711461
-21.252812	-1.932832	3.221530	0.004007	0.711489
-20.396808	-1.944911	3.231526	0.003847	0.711769
-20.248934	-1.972692	3.241523	0.003819	0.711767
-20.370956	-1.952351	3.251520	0.003842	0.711764
-19.821459	-1.941869	3.261517	0.003739	0.711981
-19.284872	-1.979745	3.271514	0.003639	0.712096
-19.151517	-2.002079	3.281510	0.003614	0.712100
-19.375944	-1.956673	3.291507	0.003656	0.712111
-18.635587	-1.947111	3.301504	0.003517	0.712393
-18.739026	-1.929376	3.311501	0.003537	0.712392
-18.516490	-1.966890	3.321498	0.003495	0.712397
-18.034093	-1.943955	3.331494	0.003405	0.712614
-17.589537	-1.973973	3.341491	0.003322	0.712713
-17.824382	-1.932791	3.351488	0.003365	0.712712
-17.467574	-1.970206	3.361485	0.003299	0.712764
-16.849906	-1.947046	3.371482	0.003183	0.713030
-16.650322	-1.983451	3.381478	0.003146	0.713029
-16.850942	-1.947503	3.391475	0.003183	0.713030
-16.286095	-1.923010	3.401472	0.003078	0.713279
-15.794539	-1.968693	3.411469	0.002986	0.713363
-15.746545	-1.975069	3.421466	0.002977	0.713368
-15.905600	-1.928536	3.431462	0.003006	0.713404
-15.229612	-1.919957	3.441459	0.002880	0.713661
-15.016374	-1.961033	3.451456	0.002840	0.713656
-14.810948	-1.996669	3.461453	0.002802	0.713658
-14.562570	-1.931681	3.471450	0.002755	0.713876
-14.261564	-1.933907	3.481446	0.002699	0.713978
-14.132248	-1.958186	3.491443	0.002675	0.713976
-14.251950	-1.893878	3.501440	0.002697	0.714062
-13.212670	-1.967895	3.511437	0.002503	0.714283
-13.147769	-1.978538	3.521434	0.002491	0.714286
-13.308116	-1.949648	3.531430	0.002520	0.714287
-12.651138	-1.938334	3.541427	0.002398	0.714542
-12.574465	-1.916682	3.551424	0.002383	0.714613
-12.220081	-1.978926	3.561421	0.002317	0.714615
-12.327227	-1.923466	3.571418	0.002337	0.714688
-11.203117	-2.008151	3.581414	0.002127	0.714917
-11.258090	-1.999054	3.591411	0.002137	0.714917
-11.627900	-1.934352	3.601408	0.002206	0.714915
-11.085422	-1.941901	3.611405	0.002104	0.715092
-10.604955	-1.953544	3.621402	0.002015	0.715239
-10.473072	-1.977217	3.631398	0.001990	0.715239
-10.749067	-1.916702	3.641395	0.002041	0.715262
-9.681905	-1.961349	3.651392	0.001842	0.715551
-9.207767	-2.045980	3.661389	0.001754	0.715551
-9.465374	-1.998784	3.671386	0.001801	0.715554
-9.304552	-2.005228	3.681382	0.001771	0.715599
-8.650487	-1.972596	3.691379	0.001649	0.715895
-8.299238	-2.036678	3.701376	0.001584	0.715892
-8.284208	-2.038671	3.711373	0.001581	0.715894
-8.244395	-2.035497	3.721370	0.001573	0.715915
-7.549146	-2.044165	3.731366	0.001443	0.716143
-7.394108	-2.071842	3.741363	0.001414	0.716144
-7.506928	-2.053785	3.751360	0.001435	0.716140
-7.388817	-2.044359	3.761357	0.001413	0.716201
-6.407770	-2.089316	3.771354	0.001230	0.716458
-6.103449	-2.143461	3.781350	0.001173	0.716459
-6.741393	-2.030028	3.791347	0.001291	0.716459
-6.483681	-2.040477	3.801344	0.001243	0.716530
-5.630809	-2.074344	3.811341	0.001084	0.716764
-5.608341	-2.078607	3.821338	0.001080	0.716764
-5.564814	-2.085713	3.831334	0.001071	0.716765
-5.294825	-2.029985	3.841331	0.001021	0.716971
-4.632876	-2.087792	3.851328	0.000898	0.717091
-4.944138	-2.032503	3.861325	0.000955	0.717091
-4.602721	-2.091198	3.871322	0.000891	0.717095
-3.992563	-2.055186	3.881318	0.000778	0.717382
-3.851659	-2.075364	3.891315	0.000751	0.717392
-3.775147	-2.091899	3.901312	0.000737	0.717387
-3.765234	-2.040266	3.911309	0.000735	0.717493
-2.938975	-2.076332	3.921306	0.000580	0.717713
-2.861096	-2.089712	3.931302	0.000566	0.717715
-3.077973	-2.051905	3.941299	0.000606	0.717713
-2.374998	-2.054313	3.951296	0.000475	0.717956
-2.077768	-2.071993	3.961293	0.000419	0.718027
-2.128094	-2.062818	3.971290	0.000428	0.718027
-1.950906	-2.055795	3.981286	0.000395	0.718104
-1.529171	-1.999818	3.991283	0.000316	0.718363
-1.756665	-1.959491	4.001280	0.000358	0.718364
-1.333706	-2.024466	4.011277	0.000279	0.718384
-1.461887	-1.866791	4.021274	0.000303	0.718651
-1.173170	-1.918108	4.031270	0.000249	0.718652
-1.101824	-1.872248	4.041267	0.000235	0.718768
-1.343467	-1.729900	4.051264	0.000280	0.718964
-0.768275	-1.822089	4.061261	0.000173	0.718985
-1.389911	-1.565223	4.071258	0.000288	0.719274
-0.691964	-1.675817	4.081254	0.000158	0.719301
-0.475924	-1.558134	4.091251	0.000118	0.719610
-0.757607	-1.494645	4.101248	0.000170	0.719636
-0.353469	-1.431397	4.111245	0.000094	0.719903
-0.788774	-1.306961	4.121242	0.000175	0.719996
-0.486096	-1.241249	4.131238	0.000118	0.720232
-0.316859	-1.166579	4.141235	0.000087	0.720439
-0.414596	-1.075821	4.151232	0.000104	0.720584
-0.072048	-0.986216	4.161229	0.000040	0.720881
-0.394823	-0.851931	4.171226	0.000100	0.721033
-0.048177	-0.828233	4.181222	0.000035	0.721201
-0.020407	-0.708086	4.191219	0.000030	0.721447
0.047973	-0.587413	4.201216	0.000017	0.721709
0.016582	-0.462411	4.211213	0.000022	0.721944
0.167869	-0.367623	4.221210	-0.000006	0.722184
0.200764	-0.250962	4.231206	-0.000013	0.722425
-0.102502	-0.049458	4.241203	0.000044	0.722715
-0.019829	0.085432	4.251200	0.000028	0.723009
0.000000	0.284004	4.261197	0.000024	0.723406

0.310269	0.839315	4.266202	-0.000034	0.724603
0.433546	2.085674	4.271206	-0.000058	0.727082
0.621485	3.908720	4.276211	-0.000095	0.730696
0.967748	6.269652	4.281216	-0.000161	0.735385
1.249840	9.138008	4.286221	-0.000215	0.740994
1.395561	12.519769	4.291226	-0.000245	0.747491
1.953756	16.279320	4.296230	-0.000351	0.754779
2.453438	20.453271	4.301235	-0.000447	0.762750
2.645780	25.095006	4.306240	-0.000486	0.771398
2.978165	30.060679	4.311245	-0.000551	0.780584
3.612747	35.331340	4.316250	-0.000673	0.790308
4.211055	40.927602	4.321254	-0.000788	0.800478
4.292649	46.913224	4.326259	-0.000807	0.811042
5.191550	53.041955	4.331264	-0.000979	0.821967
6.333519	59.404554	4.336269	-0.001196	0.833219
6.475274	66.166943	4.341274	-0.001227	0.844696
7.399897	73.020068	4.346278	-0.001403	0.856398
8.364108	80.068319	4.351283	-0.001588	0.868271
11.116508	87.030828	4.356288	-0.002105	0.880353
11.616705	94.577183	4.361293	-0.002203	0.892568
12.268865	102.238967	4.366298	-0.002330	0.904841
12.804760	110.078562	4.371302	-0.002435	0.917193
13.291013	118.024559	4.376307	-0.002530	0.929529
14.783151	125.930487	4.381312	-0.002814	0.941909
16.100961	133.972218	4.386317	-0.003064	0.954283
16.612288	142.230203	4.391322	-0.003165	0.966609
17.259491	150.559569	4.396326	-0.003291	0.978917
18.229657	158.908827	4.401331	-0.003477	0.991180
19.074886	167.325750	4.406336	-0.003640	1.003359
19.672478	175.824898	4.411341	-0.003757	1.015445
20.689690	184.288201	4.416346	-0.003952	1.027440
21.628387	192.820325	4.421350	-0.004133	1.039371
22.279184	201.415112	4.426355	-0.004260	1.051183
23.158734	210.002593	4.431360	-0.004429	1.062907
23.999801	218.624301	4.436365	-0.004591	1.074539
24.753709	227.251365	4.441370	-0.004737	1.086033
25.691259	235.877493	4.446374	-0.004918	1.097446
26.202954	244.566408	4.451379	-0.005019	1.108728
27.059337	253.200178	4.456384	-0.005184	1.119900
27.724628	261.871658	4.461389	-0.005314	1.130969
28.631113	270.482586	4.466394	-0.005488	1.141905
29.551340	279.137470	4.471398	-0.005665	1.152794
30.326663	287.758694	4.476403	-0.005815	1.163510
31.064158	296.389688	4.481408	-0.005958	1.174132
31.535876	305.038016	4.486413	-0.006052	1.184624
32.119903	313.673901	4.491418	-0.006167	1.195032
32.795271	322.265011	4.496422	-0.006298	1.205315
33.590029	330.827618	4.501427	-0.006452	1.215502
34.436933	339.375972	4.506432	-0.006615	1.225597
35.024972	347.973499	4.511437	-0.006730	1.235615
35.636657	356.510528	4.516442	-0.006850	1.245489
36.439039	365.033012	4.521446	-0.007005	1.255304
37.150080	373.531885	4.526451	-0.007143	1.264999
37.582917	382.101462	4.531456	-0.007229	1.274646
38.090811	390.604890	4.536461	-0.007329	1.284162
39.022487	399.045243	4.541466	-0.007509	1.293616
39.850611	407.505245	4.546470	-0.007668	1.303004
40.292911	416.083398	4.551475	-0.007756	1.312381
40.965287	424.555190	4.556480	-0.007887	1.321620
41.438703	432.982931	4.561485	-0.007981	1.330711
41.891355	441.417114	4.566490	-0.008071	1.339744
42.887604	449.753343	4.571494	-0.008262	1.348709
43.269716	458.185825	4.576499	-0.008339	1.357607
43.643699	466.597737	4.581504	-0.008414	1.366425
44.361699	474.947335	4.586509	-0.008553	1.375181
44.977591	483.313418	4.591514	-0.008674	1.383880
45.484837	491.720360	4.596518	-0.008774	1.392548
45.862472	500.083637	4.601523	-0.008849	1.401096
46.471700	508.423524	4.606528	-0.008968	1.409608
46.919744	516.777230	4.611533	-0.009057	1.418055
47.545625	525.075922	4.616538	-0.009179	1.426427
48.223002	533.395144	4.621542	-0.009311	1.434778
48.609404	541.723550	4.626547	-0.009389	1.443042
49.263985	550.018495	4.631552	-0.009516	1.451270
49.788753	558.333132	4.636557	-0.009619	1.459449
50.291085	566.635673	4.641562	-0.009718	1.467567
50.719089	575.013218	4.646566	-0.009804	1.475701
51.074469	583.288513	4.651571	-0.009875	1.483681
51.707379	591.554842	4.656576	-0.009999	1.491653
52.136219	599.835497	4.661581	-0.010084	1.499564
52.740210	608.086784	4.666586	-0.010202	1.507432
53.417042	616.343792	4.671590	-0.010333	1.515277
53.894810	624.585428	4.676595	-0.010428	1.523035
54.485406	632.839800	4.681600	-0.010543	1.530784
55.170616	641.071275	4.686605	-0.010676	1.538486
55.500266	649.338798	4.691610	-0.010743	1.546129
55.886231	657.640648	4.696614	-0.010821	1.553775
56.352704	665.856339	4.701619	-0.010913	1.561316
56.983895	674.074036	4.706624	-0.011036	1.568847
57.609591	682.295400	4.711629	-0.011158	1.576344
58.112545	690.509975	4.716634	-0.011257	1.583782
58.610445	698.761647	4.721638	-0.011355	1.591217
58.852586	707.021755	4.726643	-0.011406	1.598588
59.240014	715.235799	4.731648	-0.011484	1.605906
59.587423	723.480175	4.736653	-0.011554	1.613211
60.261867	731.645767	4.741658	-0.011685	1.620460
60.788168	739.859314	4.746662	-0.011788	1.627697
61.094291	748.136551	4.751667	-0.011851	1.634927
61.808221	756.276167	4.756672	-0.011989	1.642062
62.472762	764.434079	4.761677	-0.012118	1.649175
62.719096	772.671295	4.766682	-0.012170	1.656269
63.171855	780.865175	4.771686	-0.012259	1.663323
63.638081	789.051192	4.776691	-0.012352	1.670342
63.838774	797.297239	4.781696	-0.012395	1.677347
64.539854	805.419796	4.786701	-0.012530	1.684285
65.189194	813.587045	4.791706	-0.012657	1.691225
65.554662	821.802667	4.796710	-0.012730	1.698140
65.443000	830.035309	4.801715	-0.012715	1.704978
66.226127	838.187852	4.806720	-0.012866	1.711839
66.543227	846.380906	4.811725	-0.012931	1.718646
66.717895	854.547202	4.816730	-0.012969	1.725385
67.177221	862.721067	4.821734	-0.013060	1.732140
67.671913	870.854542	4.826739	-0.013157	1.738841
68.158482	878.995612	4.831744	-0.013253	1.745521
68.462846	887.187967	4.836749	-0.013315	1.752194
68.822019	895.349453	4.841754	-0.013388	1.758823
69.269030	903.494001	4.846758	-0.013476	1.765425
69.552124	911.666694	4.851763	-0.013535	1.772004
69.998179	919.829858	4.856768	-0.013623	1.778572
70.489163	927.959632	4.861773	-0.013720	1.785094
70.731353	936.166501	4.866778	-0.013770	1.791622
71.505552	944.298841	4.871782	-0.013920	1.798133
71.664554	952.440755	4.876787	-0.013955	1.804553
72.183595	960.572640	4.881792	-0.014057	1.810986
72.520935	968.737138	4.886797	-0.014125	1.817400
72.899176	976.855372	4.891802	-0.014201	1.823759
73.308005	985.002874	4.896806	-0.014283	1.830123
73.949846	993.100853	4.901811	-0.014408	1.836454
74.441410	1001.225671	4.906816	-0.014505	1.842767
74.795825	1009.379050	4.911821	-0.014576	1.849063
75.349059	1017.507869	4.916826	-0.014684	1.855342
75.842974	1025.644070	4.921830	-0.014782	1.861598
76.172358	1033.789573	4.926835	-0.014849	1.867822
76.667821	1041.962680	4.931840	-0.014946	1.874064
76.949310	1050.081032	4.936845	-0.015004	1.880220
77.464907	1058.194021	4.941850	-0.015105	1.886379
77.944964	1066.337530	4.946854	-0.015200	1.892536
78.089578	1074.482876	4.951859	-0.015233	1.898636
78.436042	1082.611629	4.956864	-0.015303	1.904727
78.810397	1090.741664	4.961869	-0.015378	1.910803
79.299262	1098.853593	4.966874	-0.015474	1.916859
79.681342	1106.975080	4.971878	-0.015551	1.922891
79.871412	1115.104978	4.976883	-0.015591	1.928888
80.093267	1123.260925	4.981888	-0.015638	1.934890
80.199538	1131.393432	4.986893	-0.015663	1.940843
80.834041	1139.462141	4.991898	-0.015787	1.946789
81.332202	1147.610959	4.996902	-0.015885	1.952760
81.461336	1155.744051	5.001907	-0.015915	1.958662
81.919415	1163.821474	5.006912	-0.016005	1.964541
82.447648	1171.900219	5.011917	-0.016109	1.970411
82.941463	1180.005165	5.016922	-0.016206	1.976278
83.495293	1188.089207	5.021926	-0.016315	1.982119
83.821341	1196.194164	5.026931	-0.016381	1.987934
84.419050	1204.318231	5.031936	-0.016498	1.993774
84.758222	1212.419840	5.036941	-0.016566	1.999553
84.950218	1220.534468	5.041946	-0.016607	2.005310
85.415539	1228.653265	5.046950	-0.016699	2.011082
85.732016	1236.764382	5.051955	-0.016764	2.016816
86.255509	1244.846268	5.056960	-0.016867	2.022534
86.635780	1252.955337	5.061965	-0.016943	2.028241
86.941407	1261.101013	5.066970	-0.017005	2.033949
87.289760	1269.204864	5.071974	-0.017075	2.039617
87.561997	1277.285200	5.076979	-0.017131	2.045244
87.940639	1285.399140	5.081984	-0.017207	2.050890
88.369839	1293.497527	5.086989	-0.017293	2.056515
88.760006	1301.587762	5.091994	-0.017371	2.062115
89.241106	1309.676570	5.096998	-0.017466	2.067708
89.368408	1317.814729	5.102003	-0.017495	2.073284
89.795047	1325.903879	5.107008	-0.017580	2.078841
90.329189	1333.956200	5.112013	-0.017684	2.084369
90.869028	1342.042416	5.117018	-0.017790	2.089906
91.263931	1350.160414	5.122022	-0.017869	2.095435
91.737439	1358.215822	5.127027	-0.017963	2.100915
92.261840	1366.307833	5.132032	-0.018066	2.106411
92.494054	1374.471925	5.137037	-0.018115	2.111911
92.825365	1382.579473	5.142042	-0.018182	2.117370
93.469082	1390.624182	5.147046	-0.018307	2.122802
93.540607	1398.719606	5.152051	-0.018326	2.128199
94.170630	1406.799322	5.157056	-0.018448	2.133625
94.381947	1414.908405	5.162061	-0.018493	2.139017
94.846712	1422.961665	5.167066	-0.018585	2.144383
95.196946	1431.063204	5.172070	-0.018656	2.149756
95.512703	1439.166676	5.177075	-0.018720	2.155113
96.029399	1447.225723	5.182080	-0.018821	2.160447
96.220158	1455.319676	5.187085	-0.018862	2.165760
96.444000	1463.433754	5.192090	-0.018909	2.171076
96.912840	1471.520429	5.197094	-0.019002	2.176384
97.163652	1479.586134	5.202099	-0.019054	2.181645
97.529056	1487.674119	5.207104	-0.019127	2.186918
97.871525	1495.776930	5.212109	-0.019197	2.192187
98.013782	1503.893802	5.217114	-0.019229	2.197433
98.222631	1511.966870	5.222118	-0.019273	2.202644
98.423216	1520.036033	5.227123	-0.019316	2.207840
98.762254	1528.127134	5.232128	-0.019384	2.213050
99.069160	1536.197535	5.237133	-0.019447	2.218232
99.376357	1544.248249	5.242138	-0.019509	2.223389
99.878693	1552.317888	5.247142	-0.019608	2.228564
100.138409	1560.418120	5.252147	-0.019662	2.233724
100.567906	1568.491624	5.257152	-0.019747	2.238870
100.970458	1576.540991	5.262157	-0.019827	2.243987
101.318173	1584.609709	5.267162	-0.019898	2.249099
101.714790	1592.730547	5.272166	-0.019977	2.254237
101.977662	1600.786061	5.277171	-0.020031	2.259311
102.548204	1608.841009	5.282176	-0.020143	2.264399
102.679228	1616.954236	5.287181	-0.020173	2.269474
103.102754	1625.098294	5.292186	-0.020257	2.274582
103.597960	1633.122063	5.297190	-0.020354	2.279610
103.426605	1641.219889	5.302195	-0.020328	2.284616
103.721958	1649.284591	5.307200	-0.020388	2.289630
104.226089	1657.340807	5.312205	-0.020487	2.294645
104.543643	1665.383504	5.317210	-0.020552	2.299626
104.742037	1673.453569	5.322214	-0.020594	2.304602
104.982156	1681.526096	5.327219	-0.020644	2.309573
105.481324	1689.600496	5.332224	-0.020743	2.314555
105.792506	1697.659924	5.337229	-0.020806	2.319502
106.036971	1705.714574	5.342234	-0.020857	2.324430
106.632599	1713.761647	5.347238	-0.020973	2.329372
106.672107	1721.880322	5.352243	-0.020986	2.334301
106.952109	1729.963474	5.357248	-0.021043	2.339217
107.103150	1738.046367	5.362253	-0.021077	2.344113
107.365880	1746.097746	5.367258	-0.021131	2.348989
107.765061	1754.213605	5.372262	-0.021211	2.353904
108.046657	1762.245427	5.377267	-0.021269	2.358749
108.313103	1770.309303	5.382272	-0.021324	2.363601
108.917885	1778.325156	5.387277	-0.021442	2.368443
109.460814	1786.370838	5.392282	-0.021548	2.373287
110.157873	1794.414791	5.397286	-0.021683	2.378132
110.451855	1802.481936	5.402291	-0.021743	2.382949
110.689306	1810.558932	5.407296	-0.021793	2.387758
111.093532	1818.663147	5.412301	-0.021874	2.392586
111.210090	1826.732626	5.417306	-0.021901	2.397361
111.617234	1834.785484	5.422310	-0.021982	2.402140
111.916915	1842.833596	5.427315	-0.022043	2.406898
112.296821	1850.932720	5.432320	-0.022119	2.411683
112.511373	1859.010071	5.437325	-0.022165	2.416432
112.807962	1867.073388	5.442330	-0.022225	2.421170
113.258190	1875.118243	5.447334	-0.022314	2.425900
113.439243	1883.204644	5.452339	-0.022353	2.430625
113.595368	1891.361791	5.457344	-0.022388	2.435379
113.734363	1899.409595	5.462349	-0.022419	2.440059
114.046636	1907.411911	5.467354	-0.022483	2.444717
114.342746	1915.481017	5.472358	-0.022543	2.449403
114.420038	1923.552954	5.477363	-0.022563	2.454066
114.795670	1931.593207	5.482368	-0.022638	2.458724
115.283404	1939.625916	5.487373	-0.022734	2.463377
115.602549	1947.678378	5.492378	-0.022799	2.468020
115.728733	1955.793404	5.497382	-0.022828	2.472675
115.991639	1963.824593	5.502387	-0.022882	2.477284
116.329513	1971.859011	5.507392	-0.022951	2.481892
116.541982	1979.899013	5.512397	-0.022996	2.486485
116.958710	1987.934511	5.517402	-0.023078	2.491082
117.299333	1996.029377	5.522406	-0.023147	2.495699
117.378255	2004.084578	5.527411	-0.023167	2.500265
117.693567	2012.131631	5.532416	-0.023231	2.504836
118.359600	2020.159083	5.537421	-0.023361	2.509412
118.666834	2028.253724	5.542426	-0.023423	2.513992
118.876185	2036.334994	5.547430	-0.023468	2.518549
119.309451	2044.323330	5.552435	-0.023554	2.523062
119.576936	2052.389811	5.557440	-0.023609	2.527598
119.780822	2060.475711	5.562445	-0.023652	2.532133
120.033239	2068.539548	5.567450	-0.023705	2.536650
120.497681	2076.591558	5.572454	-0.023797	2.541168
120.702273	2084.629048	5.577459	-0.023840	2.545652
121.005570	2092.695932	5.582464	-0.023902	2.550150
121.363071	2100.755178	5.587469	-0.023974	2.554640
121.510289	2108.818936	5.592474	-0.024007	2.559111
121.891490	2116.854670	5.597478	-0.024083	2.563574
122.348260	2124.871896	5.602483	-0.024173	2.568024
122.340618	2132.988645	5.607488	-0.024177	2.572489
122.649568	2141.041953	5.612493	-0.024240	2.576933
122.979647	2149.069101	5.617498	-0.024307	2.581357
123.326895	2157.120071	5.622502	-0.024377	2.585787
123.482054	2165.197901	5.627507	-0.024411	2.590211
123.759897	2173.444785	5.632512	-0.024468	2.594729
124.415499	2181.368542	5.637517	-0.024596	2.599087
124.638764	2189.378119	5.642522	-0.024643	2.603456
124.629321	2197.451467	5.647526	-0.024646	2.607837
124.830038	2205.484679	5.652531	-0.024689	2.612202
125.390261	2213.506932	5.657536	-0.024799	2.616579
125.610106	2221.554027	5.662541	-0.024845	2.620938
125.705535	2229.590001	5.667546	-0.024868	2.625276
126.233235	2237.622711	5.672550	-0.024972	2.629634
126.375960	2245.705325	5.677555	-0.025004	2.633986
126.799245	2253.734650	5.682560	-0.025088	2.638320
127.130762	2261.766506	5.687565	-0.025155	2.642643
127.313859	2269.807659	5.692570	-0.025194	2.646953
127.314211	2277.915670	5.697574	-0.025200	2.651281
127.491364	2285.978444	5.702579	-0.025238	2.655589
127.931774	2293.998893	5.707584	-0.025326	2.659884
128.067892	2302.045426	5.712589	-0.025356	2.664166
128.330357	2310.079063	5.717594	-0.025410	2.668443
128.834677	2318.156072	5.722598	-0.025510	2.672751
128.866075	2326.219066	5.727603	-0.025521	2.677015
129.102956	2334.241718	5.732608	-0.025570	2.681264
129.502547	2342.251703	5.737613	-0.025650	2.685510
129.708825	2350.286579	5.742618	-0.025694	2.689749
129.773862	2358.401796	5.747622	-0.025711	2.694015
130.028443	2366.423773	5.752627	-0.025764	2.698238
130.448596	2374.438649	5.757632	-0.025848	2.702460
130.420234	2382.520522	5.762637	-0.025848	2.706683
130.637612	2390.553955	5.767642	-0.025894	2.710890
131.022395	2398.637018	5.772646	-0.025971	2.715125
131.079369	2406.649417	5.777651	-0.025987	2.719298
131.482775	2414.673323	5.782656	-0.026067	2.723491
131.804416	2422.723746	5.787661	-0.026132	2.727686
131.904927	2430.778540	5.792666	-0.026156	2.731864
132.207922	2438.860477	5.797670	-0.026218	2.736061
132.362139	2446.881782	5.802675	-0.026252	2.740212
132.924814	2454.869670	5.807680	-0.026362	2.744364
133.059634	2462.976131	5.812685	-0.026393	2.748545
133.270012	2471.070954	5.817690	-0.026437	2.752717
133.467702	2479.164455	5.822694	-0.026480	2.756883
133.771433	2487.144493	5.827699	-0.026542	2.760990
134.088885	2495.138045	5.832704	-0.026606	2.765098
134.392260	2503.186293	5.837709	-0.026668	2.769228
134.734988	2511.210916	5.842714	-0.026737	2.773341
135.213801	2519.255157	5.847718	-0.026832	2.777467
135.300922	2527.288260	5.852723	-0.026853	2.781557
135.613970	2535.331081	5.857728	-0.026917	2.785660
135.979272	2543.377440	5.862733	-0.026990	2.789761
135.878197	2551.485351	5.867738	-0.026977	2.793860
136.174258	2559.508699	5.872742	-0.027037	2.797934
136.330444	2567.532768	5.877747	-0.027072	2.801994
136.561445	2575.562461	5.882752	-0.027120	2.806055
136.962641	2583.604280	5.887757	-0.027200	2.810126
137.177587	2591.662520	5.892762	-0.027245	2.814188
137.395537	2599.712271	5.897766	-0.027291	2.818241
137.487642	2607.755048	5.902771	-0.027314	2.822277
137.783892	2615.799271	5.907776	-0.027374	2.826320
137.924261	2623.858518	5.912781	-0.027406	2.830355
138.164751	2631.920501	5.917786	-0.027456	2.834392
138.469011	2639.948027	5.922790	-0.027518	2.838410
139.015445	2647.916407	5.927795	-0.027625	2.842405
139.463937	2655.970865	5.932800	-0.027714	2.846433
139.741749	2664.009619	5.937805	-0.027771	2.850437
139.856714	2672.104000	5.942810	-0.027798	2.854454
140.100612	2680.135399	5.947814	-0.027849	2.858442
140.151825	2688.147264	5.952819	-0.027863	2.862403
140.673308	2696.182248	5.957824	-0.027966	2.866396
141.050380	2704.222664	5.962829	-0.028042	2.870379
141.122523	2712.283684	5.967834	-0.028060	2.874349
141.526399	2720.311995	5.972838	-0.028141	2.878316
141.677243	2728.357428	5.977843	-0.028174	2.882272
141.964982	2736.370773	5.982848	-0.028233	2.886214
142.365504	2744.391695	5.987853	-0.028313	2.890161
142.544547	2752.479603	5.992858	-0.028352	2.894122
142.643245	2760.547225	5.997862	-0.028376	2.898065
142.772637	2768.584050	6.002867	-0.028405	2.901988
143.131865	2776.587957	6.007872	-0.028477	2.905902
143.457507	2784.632899	6.012877	-0.028543	2.909829
143.597382	2792.773604	6.017882	-0.028575	2.913788
144.290455	2800.766383	6.022886	-0.028709	2.917698
144.638564	2808.743356	6.027891	-0.028779	2.921578
144.764118	2816.765056	6.032896	-0.028808	2.925462
145.084332	2824.796395	6.037901	-0.028873	2.929356
145.335617	2832.854504	6.042906	-0.028925	2.933254
145.505117	2840.918057	6.047910	-0.028962	2.937144
145.927329	2848.920896	6.052915	-0.029046	2.941014
146.147477	2856.941351	6.057920	-0.029092	2.944877
146.529476	2864.984996	6.062925	-0.029169	2.948754
146.609949	2873.057507	6.067930	-0.029189	2.952624
146.786523	2881.117282	6.072934	-0.029227	2.956487
147.137190	2889.093182	6.077939	-0.029298	2.960315
147.610812	2897.127359	6.082944	-0.029392	2.964172
147.839143	2905.171553	6.087949	-0.029439	2.968015
148.085865	2913.211869	6.092954	-0.029491	2.971853
148.413364	2921.298837	6.097958	-0.029557	2.975712
148.562416	2929.298900	6.102963	-0.029590	2.979516
148.625626	2937.355941	6.107968	-0.029607	2.983338
148.947298	2945.386122	6.112973	-0.029673	2.987155
149.247947	2953.423684	6.117978	-0.029734	2.990969
149.581402	2961.496671	6.122982	-0.029801	2.994797
149.964071	2969.487538	6.127987	-0.029878	2.998584
150.122933	2977.521492	6.132992	-0.029913	3.002375
150.044528	2985.585899	6.137997	-0.029904	3.006164
150.200307	2993.591397	6.143002	-0.029938	3.009932
150.520414	3001.675770	6.148006	-0.030003	3.013740
150.503971	3009.709590	6.153011	-0.030005	3.017503
150.811219	3017.721784	6.158016	-0.030068	3.021267
151.253851	3025.728751	6.163021	-0.030156	3.025031
151.419830	3033.757854	6.168026	-0.030192	3.028787
151.735828	3041.829755	6.173030	-0.030256	3.032565
151.832672	3049.888214	6.178035	-0.030279	3.036322
152.045508	3057.898414	6.183040	-0.030324	3.040057
152.065347	3065.940439	6.188045	-0.030333	3.043793
152.530199	3073.923808	6.193050	-0.030425	3.047519
152.696589	3082.015185	6.198054	-0.030462	3.051275
152.848579	3090.055316	6.203059	-0.030495	3.055003
153.183952	3098.059610	6.208064	-0.030563	3.058718
153.501865	3106.089805	6.213069	-0.030628	3.062440
153.637564	3114.124742	6.218074	-0.030658	3.066151
153.775057	3122.186269	6.223078	-0.030689	3.069869
154.036399	3130.282470	6.228083	-0.030743	3.073605
154.284198	3138.314547	6.233088	-0.030795	3.077306
154.582527	3146.318652	6.238093	-0.030856	3.080992
154.690245	3154.286924	6.243098	-0.030881	3.084649
155.055854	3162.327536	6.248102	-0.030955	3.088346
155.330609	3170.352920	6.253107	-0.031011	3.092027
155.502357	3178.429109	6.258112	-0.031048	3.095723
155.930129	3186.415505	6.263117	-0.031133	3.099385
156.181444	3194.434642	6.268122	-0.031185	3.103049
156.372182	3202.501001	6.273126	-0.031226	3.106728
156.628993	3210.518226	6.278131	-0.031280	3.110383
156.895751	3218.571562	6.283136	-0.031335	3.114050
157.149270	3226.597258	6.288141	-0.031387	3.117700
157.392093	3234.643900	6.293146	-0.031438	3.121355
157.591906	3242.643560	6.298150	-0.031480	3.124982
157.884619	3250.680141	6.303155	-0.031540	3.128625
157.955625	3258.755606	6.308160	-0.031559	3.132272
158.117054	3266.793557	6.313165	-0.031594	3.135902
158.263449	3274.796583	6.318170	-0.031627	3.139512
158.495097	3282.843659	6.323174	-0.031675	3.143140
158.755340	3290.857039	6.328179	-0.031729	3.146751
159.178018	3298.884182	6.333184	-0.031813	3.150371
159.557527	3306.943087	6.338189	-0.031889	3.153999
159.801368	3314.964568	6.343194	-0.031940	3.157599
160.342219	3322.975059	6.348198	-0.032046	3.161204
160.539516	3330.956008	6.353203	-0.032088	3.164777
160.576018	3339.020361	6.358208	-0.032100	3.168375
160.707665	3347.101610	6.363213	-0.032130	3.171982
160.918533	3355.142433	6.368218	-0.032175	3.175569
161.156465	3363.179335	6.373222	-0.032224	3.179152
161.533948	3371.150924	6.378227	-0.032300	3.182708
161.911938	3379.198482	6.383232	-0.032376	3.186293
162.232650	3387.226190	6.388237	-0.032441	3.189863
162.389195	3395.308258	6.393242	-0.032475	3.193446
162.792944	3403.365520	6.398246	-0.032556	3.197024
162.960573	3411.331192	6.403251	-0.032592	3.200549
163.241100	3419.365223	6.408256	-0.032650	3.204104
163.775832	3427.398625	6.413261	-0.032755	3.207665
163.988425	3435.433095	6.418266	-0.032800	3.211209
164.154644	3443.498661	6.423270	-0.032836	3.214761
164.317306	3451.517366	6.428275	-0.032872	3.218289
164.754770	3459.526480	6.433280	-0.032958	3.221820
164.929219	3467.553368	6.438285	-0.032996	3.225343
164.975536	3475.593875	6.443290	-0.033010	3.228864
165.364879	3483.661456	6.448294	-0.033088	3.232407
165.529920	3491.715170	6.453299	-0.033124	3.235930
165.741728	3499.686072	6.458304	-0.033169	3.239416
165.934528	3507.731940	6.463309	-0.033210	3.242929
166.145714	3515.730404	6.468314	-0.033255	3.246419
166.280804	3523.771138	6.473318	-0.033285	3.249920
166.592307	3531.795146	6.478323	-0.033349	3.253417
166.698362	3539.841642	6.483328	-0.033374	3.256913
167.044830	3547.853342	6.488333	-0.033444	3.260398
167.201165	3555.860750	6.493338	-0.033478	3.263871
167.450742	3563.920331	6.498342	-0.033530	3.267366
167.716680	3571.927174	6.503347	-0.033585	3.270835
167.995847	3579.994305	6.508352	-0.033642	3.274327
168.414803	3588.014131	6.513357	-0.033726	3.277800
168.512666	3596.032340	6.518362	-0.033749	3.281257
168.669973	3604.042838	6.523366	-0.033784	3.284708
168.834734	3612.082988	6.528371	-0.033820	3.288169
169.126733	3620.125439	6.533376	-0.033879	3.291633
169.417713	3628.167129	6.538381	-0.033939	3.295092
169.458084	3636.181339	6.543386	-0.033952	3.298526
169.865860	3644.210785	6.548390	-0.034033	3.301977
170.194187	3652.199591	6.553395	-0.034100	3.305404
170.195242	3660.286454	6.558400	-0.034105	3.308857
170.256230	3668.349399	6.563405	-0.034122	3.312298
170.538838	3676.369040	6.568410	-0.034180	3.315726
170.937376	3684.369351	6.573414	-0.034259	3.319146
170.981723	3692.362807	6.578419	-0.034273	3.322547
171.137995	3700.395896	6.583424	-0.034307	3.325965
171.587636	3708.413998	6.588429	-0.034397	3.329384
171.773779	3716.445769	6.593434	-0.034437	3.332795
172.026992	3724.517675	6.598438	-0.034489	3.336222
172.363613	3732.487420	6.603443	-0.034557	3.339606
172.552759	3740.514359	6.608448	-0.034598	3.343005
172.806124	3748.576594	6.613453	-0.034650	3.346418
172.771027	3756.588265	6.618458	-0.034649	3.349795
173.070665	3764.682391	6.623462	-0.034710	3.353216
173.262852	3772.712477	6.628467	-0.034751	3.356602
173.394208	3780.678693	6.633472	-0.034781	3.359956
173.739268	3788.688300	6.638477	-0.034851	3.363333
173.781353	3796.755672	6.643482	-0.034864	3.366719
174.163600	3804.791950	6.648486	-0.034940	3.370101
174.516282	3812.836005	6.653491	-0.035011	3.373482
174.700898	3820.880821	6.658496	-0.035051	3.376854
174.848290	3828.887572	6.663501	-0.035084	3.380205
175.390064	3836.836329	6.668506	-0.035190	3.383542
175.478647	3844.938241	6.673510	-0.035212	3.386924
175.548955	3852.947118	6.678515	-0.035230	3.390264
175.965080	3861.038678	6.683520	-0.035313	3.393646
176.218870	3869.095671	6.688525	-0.035366	3.397005
176.419604	3877.026810	6.693530	-0.035409	3.400306
176.629431	3885.054575	6.698534	-0.035453	3.403645
176.975440	3893.077582	6.703539	-0.035523	3.406983
176.989936	3901.092939	6.708544	-0.035531	3.410303
177.214606	3909.135091	6.713549	-0.035578	3.413639
177.345149	3917.164978	6.718554	-0.035608	3.416962
177.706528	3925.175559	6.723558	-0.035680	3.420283
178.057099	3933.163943	6.728563	-0.035751	3.423590
178.324544	3941.219279	6.733568	-0.035806	3.426919
178.506530	3949.248554	6.738573	-0.035845	3.430231
178.478805	3957.305699	6.743578	-0.035845	3.433545
178.883366	3965.351668	6.748582	-0.035926	3.436864
179.067444	3973.322191	6.753587	-0.035966	3.440143
179.326848	3981.358327	6.758592	-0.036019	3.443448
179.515760	3989.399578	6.763597	-0.036060	3.446749
179.687572	3997.424060	6.768602	-0.036097	3.450039
180.024010	4005.456904	6.773606	-0.036165	3.453336
180.332432	4013.522753	6.778611	-0.036228	3.456641
180.518396	4021.504423	6.783616	-0.036268	3.459905
180.916957	4029.558078	6.788621	-0.036348	3.463202
180.835573	4037.583150	6.793626	-0.036338	3.466469
181.180915	4045.602087	6.798630	-0.036407	3.469744
181.268051	4053.649834	6.803635	-0.036429	3.473019
181.665791	4061.690866	6.808640	-0.036508	3.476299
182.088588	4069.653840	6.813645	-0.036592	3.479544
182.371774	4077.639196	6.818650	-0.036651	3.482791
182.622929	4085.689378	6.823654	-0.036703	3.486060
182.647289	4093.708508	6.828659	-0.036713	3.489306
182.976327	4101.748612	6.833664	-0.036779	3.492568
183.456962	4109.769994	6.838669	-0.036874	3.495823
183.549820	4117.799546	6.843674	-0.036897	3.499066
183.640724	4125.856115	6.848678	-0.036919	3.502318
183.842856	4133.817874	6.853683	-0.036962	3.505531
184.230059	4141.864471	6.858688	-0.037039	3.508781
184.445922	4149.948872	6.863693	-0.037085	3.512039
184.570586	4157.925746	6.868698	-0.037113	3.515247
184.986559	4165.982045	6.873702	-0.037196	3.518493
185.185501	4173.998526	6.878707	-0.037239	3.521713
185.276751	4181.967415	6.883712	-0.037261	3.524908
185.470833	4190.043541	6.888717	-0.037302	3.528146
185.783895	4198.067478	6.893722	-0.037366	3.531364
186.081890	4206.125816	6.898726	-0.037427	3.534592
186.431015	4214.111938	6.903731	-0.037497	3.537790
186.466979	4222.157758	6.908736	-0.037509	3.540999
186.555802	4230.202272	6.913741	-0.037531	3.544207
186.745932	4238.217582	6.918746	-0.037572	3.547403
187.129688	4246.249471	6.923750	-0.037649	3.550608
187.241139	4254.389842	6.928755	-0.037675	3.553846
187.428016	4262.395238	6.933760	-0.037715	3.557029
187.871408	4270.334754	6.938765	-0.037803	3.560191
188.014372	4278.330300	6.943770	-0.037835	3.563363
188.209334	4286.379747	6.948774	-0.037877	3.566555
188.314728	4294.352991	6.953779	-0.037901	3.569712
188.779921	4302.392620	6.958784	-0.037993	3.572902
188.973122	4310.462490	6.963789	-0.038035	3.576094
189.042079	4318.430644	6.968794	-0.038053	3.579239
189.468002	4326.447536	6.973798	-0.038138	3.582411
189.685892	4334.443027	6.978803	-0.038183	3.585565
189.713495	4342.512471	6.983808	-0.038194	3.588741
189.795142	4350.567745	6.988813	-0.038215	3.591909
190.104267	4358.559911	6.993818	-0.038277	3.595056
190.503551	4366.563978	6.998822	-0.038357	3.598208
190.561174	4374.581893	7.003827	-0.038373	3.601353
190.817708	4382.569692	7.008832	-0.038426	3.604489
191.141596	4390.651618	7.013837	-0.038492	3.607660
191.269164	4398.659522	7.018842	-0.038521	3.610795
191.620899	4406.697145	7.023846	-0.038592	3.613944
191.929043	4414.733784	7.028851	-0.038655	3.617089
192.099307	4422.721479	7.033856	-0.038692	3.620209
192.478592	4430.743335	7.038861	-0.038768	3.623344
192.516874	4438.774242	7.043866	-0.038780	3.626472
192.750417	4446.818715	7.048870	-0.038829	3.629607
192.898683	4454.882551	7.053875	-0.038862	3.632745
193.237527	4462.913014	7.058880	-0.038930	3.635872
193.510650	4470.918008	7.063885	-0.038987	3.638984
193.669261	4478.937795	7.068890	-0.039021	3.642097
193.958349	4486.920970	7.073894	-0.039081	3.645196
194.061074	4494.960842	7.078899	-0.039105	3.648310
194.495069	4502.984436	7.083904	-0.039191	3.651423
194.690464	4511.063507	7.088909	-0.039233	3.654549
194.827884	4519.063654	7.093914	-0.039264	3.657640
195.098400	4527.083589	7.098918	-0.039320	3.660739
195.049058	4535.096960	7.103923	-0.039316	3.663825
195.371718	4543.125559	7.108928	-0.039381	3.666924
195.554117	4551.145244	7.113933	-0.039421	3.670013
195.669234	4559.173792	7.118938	-0.039447	3.673102
195.770466	4567.236103	7.123942	-0.039472	3.676200
195.987894	4575.180387	7.128947	-0.039517	3.679253
196.069258	4583.226673	7.133952	-0.039538	3.682340
196.221871	4591.238394	7.138957	-0.039572	3.685412
196.514801	4599.265678	7.143962	-0.039631	3.688491
196.934569	4607.319332	7.148966	-0.039715	3.691581
196.991278	4615.343791	7.153971	-0.039731	3.694648
197.052895	4623.358269	7.158976	-0.039748	3.697709
197.493835	4631.350880	7.163981	-0.039835	3.700768
197.494020	4639.379449	7.168986	-0.039841	3.703828
197.825621	4647.443470	7.173990	-0.039908	3.706906
198.104321	4655.404437	7.178995	-0.039965	3.709942
198.363782	4663.491596	7.184000	-0.040019	3.713022
198.633628	4671.583291	7.189005	-0.040074	3.716102
198.764519	4679.540009	7.194010	-0.040104	3.719125
199.042833	4687.559036	7.199014	-0.040161	3.722172
199.158834	4695.503469	7.204019	-0.040188	3.725185
199.140634	4703.575007	7.209024	-0.040190	3.728240
199.430415	4711.600067	7.214029	-0.040249	3.731283
199.611663	4719.585685	7.219034	-0.040288	3.734305
199.831311	4727.651565	7.224038	-0.040335	3.737356
199.947116	4735.637035	7.229043	-0.040361	3.740372
200.172758	4743.648740	7.234048	-0.040409	3.743398
200.485683	4751.696488	7.239053	-0.040472	3.746437
200.703627	4759.706954	7.244058	-0.040518	3.749457
201.005377	4767.777823	7.249062	-0.040580	3.752500
201.224109	4775.787301	7.254067	-0.040626	3.755514
201.359753	4783.815851	7.259072	-0.040657	3.758532
201.691627	4791.839045	7.264077	-0.040724	3.761550
201.624485	4799.799595	7.269082	-0.040716	3.764533
201.945842	4807.897329	7.274086	-0.040782	3.767573
202.317795	4815.884399	7.279091	-0.040856	3.770571
202.591177	4823.916455	7.284096	-0.040913	3.773581
202.615175	4831.994139	7.289101	-0.040922	3.776600
202.799649	4839.929925	7.294106	-0.040962	3.779567
203.109910	4847.994353	7.299110	-0.041025	3.782583
203.010968	4856.005700	7.304115	-0.041012	3.785567
203.048611	4864.054718	7.309120	-0.041024	3.788566
203.553075	4872.071893	7.314125	-0.041124	3.791561
203.791297	4880.104455	7.319130	-0.041173	3.794553
203.861295	4888.160819	7.324134	-0.041192	3.797549
203.980737	4896.106320	7.329139	-0.041219	3.800501
204.119693	4904.101547	7.334144	-0.041251	3.803471
204.347101	4912.140121	7.339149	-0.041298	3.806456
204.628338	4920.124690	7.344154	-0.041356	3.809419
204.919695	4928.185908	7.349158	-0.041416	3.812409
205.094924	4936.207006	7.354163	-0.041454	3.815380
205.385278	4944.191560	7.359168	-0.041513	3.818336
205.625841	4952.247844	7.364173	-0.041563	3.821316
205.788057	4960.221838	7.369178	-0.041599	3.824262
205.912227	4968.294836	7.374182	-0.041627	3.827241
206.137939	4976.286266	7.379187	-0.041674	3.830190
206.403877	4984.334318	7.384192	-0.041729	3.833158
206.517577	4992.386159	7.389197	-0.041756	3.836122
206.577344	5000.345303	7.394202	-0.041772	3.839048
206.975213	5008.416894	7.399206	-0.041852	3.842021
207.281231	5016.391034	7.404211	-0.041914	3.844953
207.352741	5024.442175	7.409216	-0.041933	3.847907
207.580353	5032.459476	7.414221	-0.041980	3.850849
207.894780	5040.482555	7.419226	-0.042044	3.853793
208.040366	5048.548388	7.424230	-0.042077	3.856747
208.114732	5056.502151	7.429235	-0.042096	3.859656
208.421671	5064.534932	7.434240	-0.042158	3.862596
208.625067	5072.570117	7.439245	-0.042202	3.865533
208.890718	5080.617601	7.444250	-0.042257	3.868473
209.193763	5088.677909	7.449254	-0.042318	3.871417
209.352260	5096.861080	7.454259	-0.042353	3.874400
209.458141	5104.822534	7.459264	-0.042378	3.877299
210.099978	5112.794417	7.464269	-0.042503	3.880210
210.080468	5120.757409	7.469274	-0.042505	3.883103
210.442862	5128.739927	7.474278	-0.042578	3.886008
210.522041	5136.785511	7.479283	-0.042598	3.888928
210.745782	5144.801256	7.484288	-0.042645	3.891838
211.097073	5152.857037	7.489293	-0.042715	3.894763
211.198458	5160.845612	7.494298	-0.042740	3.897656
211.233467	5168.846169	7.499302	-0.042752	3.900551
211.568408	5176.850331	7.504307	-0.042819	3.903450
211.668466	5184.858712	7.509312	-0.042843	3.906344
212.020869	5192.911350	7.514317	-0.042914	3.909256
212.190394	5200.915298	7.519322	-0.042951	3.912146
212.327694	5208.957200	7.524326	-0.042982	3.915046
212.381662	5216.967673	7.529331	-0.042997	3.917931
212.567754	5224.968809	7.534336	-0.043037	3.920814
212.791466	5232.985341	7.539341	-0.043084	3.923700
212.988503	5240.973560	7.544346	-0.043126	3.926573
213.154318	5249.011888	7.549350	-0.043163	3.929462
213.248421	5257.067569	7.554355	-0.043185	3.932354
213.273546	5265.077715	7.559360	-0.043196	3.935226
213.630321	5273.123778	7.564365	-0.043267	3.938114
213.828310	5281.086767	7.569370	-0.043309	3.940968
214.048246	5289.134016	7.574374	-0.043356	3.943850
214.016072	5297.145215	7.579379	-0.043355	3.946713
214.414554	5305.138954	7.584384	-0.043435	3.949575
214.803334	5313.195136	7.589389	-0.043512	3.952457
214.859982	5321.203109	7.594394	-0.043528	3.955314
214.840044	5329.251202	7.599398	-0.043530	3.958182
215.094750	5337.244823	7.604403	-0.043583	3.961033
215.363043	5345.181369	7.609408	-0.043638	3.963862
215.545382	5353.259464	7.614413	-0.043677	3.966737
215.667777	5361.255772	7.619418	-0.043705	3.969581
216.006267	5369.331408	7.624422	-0.043774	3.972454
215.914532	5377.360735	7.629427	-0.043762	3.975302
216.248780	5385.368274	7.634432	-0.043830	3.978146
216.585176	5393.368374	7.639437	-0.043898	3.980986
216.698881	5401.377433	7.644442	-0.043924	3.983824
217.171197	5409.406876	7.649446	-0.044017	3.986673
217.213356	5417.437860	7.654451	-0.044031	3.989513
217.449168	5425.455271	7.659456	-0.044080	3.992349
217.862926	5433.530674	7.664461	-0.044162	3.995207
218.036984	5441.512076	7.669466	-0.044200	3.998025
218.184204	5449.549108	7.674470	-0.044233	4.000861
218.362830	5457.572792	7.679475	-0.044271	4.003690
218.557225	5465.566944	7.684480	-0.044313	4.006508
218.787383	5473.613185	7.689485	-0.044361	4.009342
218.645362	5481.645922	7.694490	-0.044340	4.012163
218.941517	5489.675904	7.699494	-0.044401	4.014989
219.147263	5497.705796	7.704499	-0.044444	4.017811
219.383772	5505.681346	7.709504	-0.044494	4.020612
219.552943	5513.734051	7.714509	-0.044530	4.023438
219.648382	5521.722532	7.719514	-0.044553	4.026237
220.012402	5529.741801	7.724518	-0.044627	4.029050
220.194667	5537.751301	7.729523	-0.044666	4.031855
220.448336	5545.868885	7.734528	-0.044719	4.034696
220.660470	5553.884970	7.739533	-0.044763	4.037499
220.483567	5561.816459	7.744538	-0.044736	4.040265
220.757283	5569.827746	7.749542	-0.044792	4.043064
221.283980	5577.828892	7.754547	-0.044895	4.045860
221.198524	5585.838529	7.759552	-0.044885	4.048649
221.424912	5593.906409	7.764557	-0.044932	4.051461
221.598525	5601.917502	7.769562	-0.044970	4.054250
221.846731	5609.941954	7.774566	-0.045022	4.057043
221.988677	5617.906202	7.779571	-0.045053	4.059812
222.015039	5625.959757	7.784576	-0.045064	4.062608
222.388145	5633.987943	7.789581	-0.045138	4.065398
222.486361	5641.991278	7.794586	-0.045162	4.068174
222.740022	5650.013822	7.799590	-0.045215	4.070956
222.754733	5658.027903	7.804595	-0.045223	4.073731
223.137986	5666.083606	7.809600	-0.045299	4.076523
223.510744	5674.076752	7.814605	-0.045374	4.079291
223.613059	5682.061550	7.819610	-0.045399	4.082051
223.678544	5690.052316	7.824614	-0.045416	4.084811
223.778470	5698.135916	7.829619	-0.045440	4.087601
224.171221	5706.097974	7.834624	-0.045518	4.090351
224.339115	5714.163833	7.839629	-0.045555	4.093132
224.328674	5722.155808	7.844634	-0.045558	4.095883
224.643098	5730.190892	7.849638	-0.045622	4.098652
224.907220	5738.188918	7.854643	-0.045677	4.101405
225.047116	5746.185233	7.859648	-0.045708	4.104154
225.163015	5754.256080	7.864653	-0.045735	4.106927
225.296473	5762.235312	7.869658	-0.045765	4.109667
225.713195	5770.317054	7.874662	-0.045848	4.112443
225.918051	5778.376596	7.879667	-0.045892	4.115207
225.978881	5786.380278	7.884672	-0.045909	4.117949
226.198162	5794.390018	7.889677	-0.045955	4.120692
226.274441	5802.381084	7.894682	-0.045974	4.123426
226.622624	5810.374220	7.899686	-0.046044	4.126162
226.838368	5818.444255	7.904691	-0.046090	4.128920
226.986473	5826.445295	7.909696	-0.046123	4.131653
227.315741	5834.505802	7.914701	-0.046190	4.134406
227.383992	5842.514928	7.919706	-0.046208	4.137136
227.591933	5850.508963	7.924710	-0.046252	4.139861
227.750181	5858.568791	7.929715	-0.046286	4.142607
228.076008	5866.497013	7.934720	-0.046352	4.145307
228.240259	5874.578448	7.939725	-0.046388	4.148056
228.251646	5882.591419	7.944730	-0.046396	4.150778
228.394392	5890.626410	7.949734	-0.046428	4.153507
228.633702	5898.610132	7.954739	-0.046478	4.156219
228.749329	5906.639208	7.959744	-0.046505	4.158942
228.979486	5914.685492	7.964749	-0.046553	4.161671
229.076909	5922.630826	7.969754	-0.046576	4.164362
229.407164	5930.693745	7.974758	-0.046643	4.167093
229.437921	5938.726552	7.979763	-0.046654	4.169810
229.587552	5946.718272	7.984768	-0.046687	4.172512
229.821853	5954.763396	7.989773	-0.046736	4.175231
229.999928	5962.757357	7.994778	-0.046775	4.177931
229.925901	5970.809920	7.999782	-0.046766	4.180646
230.181533	5978.800806	8.004787	-0.046819	4.183342
230.358884	5986.799406	8.009792	-0.046858	4.186037
230.590454	5994.808981	8.014797	-0.046906	4.188736
230.722510	6002.866819	8.019802	-0.046936	4.191448
231.118218	6010.957161	8.024806	-0.047015	4.194171
231.129557	6018.991194	8.029811	-0.047023	4.196870
231.294262	6026.942978	8.034816	-0.047059	4.199541
231.556174	6034.943521	8.039821	-0.047113	4.202228
231.865818	6042.854726	8.044826	-0.047176	4.204884
232.031907	6050.912340	8.049830	-0.047212	4.207585
232.196052	6058.934229	8.054835	-0.047248	4.210273
232.372299	6066.971230	8.059840	-0.047286	4.212964
232.694258	6075.016685	8.064845	-0.047351	4.215658
232.772323	6083.006254	8.069850	-0.047371	4.218329
233.298165	6091.004912	8.074854	-0.047474	4.221005
233.344749	6099.014104	8.079859	-0.047488	4.223679
233.453238	6107.068778	8.084864	-0.047514	4.226367
233.653563	6115.067966	8.089869	-0.047557	4.229035
233.736336	6123.119636	8.094874	-0.047577	4.231718
233.993563	6131.126599	8.099878	-0.047631	4.234386
234.079735	6139.187547	8.104883	-0.047652	4.237069
234.255001	6147.123475	8.109888	-0.047690	4.239709
234.520956	6155.211406	8.114893	-0.047745	4.242399
234.419699	6163.154596	8.119898	-0.047731	4.245036
234.681214	6171.238857	8.124902	-0.047785	4.247721
235.062159	6179.198061	8.129907	-0.047862	4.250364
235.066592	6187.281593	8.134912	-0.047868	4.253043
235.381978	6195.318737	8.139917	-0.047932	4.255708
235.655123	6203.291395	8.144922	-0.047988	4.258350
235.724245	6211.261157	8.149926	-0.048006	4.260987
235.924654	6219.341168	8.154931	-0.048049	4.263660
236.087815	6227.307244	8.159936	-0.048085	4.266294
236.376787	6235.361219	8.164941	-0.048144	4.268955
236.252880	6243.375759	8.169946	-0.048126	4.271599
236.723774	6251.481822	8.174950	-0.048219	4.274276
237.088322	6259.507657	8.179955	-0.048292	4.276924
236.844280	6267.429239	8.184960	-0.048252	4.279531
237.124496	6275.470021	8.189965	-0.048310	4.282180
237.415437	6283.425461	8.194970	-0.048369	4.284800
237.542127	6291.481943	8.199974	-0.048398	4.287449
237.554995	6299.491021	8.204979	-0.048406	4.290081
237.873772	6307.547335	8.209984	-0.048471	4.292729
238.103134	6315.588945	8.214989	-0.048519	4.295369
238.036753	6323.605264	8.219994	-0.048512	4.297998
238.381310	6331.571368	8.224998	-0.048581	4.300611
238.576647	6339.625926	8.230003	-0.048623	4.303251
238.736182	6347.609996	8.235008	-0.048658	4.305866
238.830162	6355.655816	8.240013	-0.048681	4.308498
239.013979	6363.663551	8.245018	-0.048720	4.311118
239.176306	6371.725454	8.250022	-0.048756	4.313753
239.379728	6379.745566	8.255027	-0.048799	4.316373
239.488460	6387.700896	8.260032	-0.048825	4.318970
239.621877	6395.721826	8.265037	-0.048855	4.321587
239.669892	6403.689112	8.270042	-0.048869	4.324184
239.956645	6411.755949	8.275046	-0.048928	4.326814
240.228872	6419.743699	8.280051	-0.048984	4.329416
240.373692	6427.822487	8.285056	-0.049016	4.332045
240.468233	6435.842915	8.290061	-0.049039	4.334654
240.739282	6443.837774	8.295066	-0.049095	4.337254
240.863564	6451.803917	8.300070	-0.049123	4.339841
241.066273	6459.840686	8.305075	-0.049166	4.342451
241.116857	6467.815055	8.310080	-0.049181	4.345038
241.464101	6475.881940	8.315085	-0.049251	4.347655
241.520225	6483.897689	8.320090	-0.049267	4.350252
241.760316	6491.972662	8.325094	-0.049317	4.352868
242.195628	6500.027721	8.330099	-0.049404	4.355477
242.364972	6507.971026	8.335104	-0.049440	4.358047
242.408041	6515.996772	8.340109	-0.049454	4.360641
242.474299	6523.968891	8.345114	-0.049471	4.363216
242.892314	6531.973326	8.350118	-0.049555	4.365803
243.128537	6539.978155	8.355123	-0.049604	4.368386
243.086580	6548.007219	8.360128	-0.049601	4.370975
243.518584	6556.049315	8.365133	-0.049687	4.373569
243.606155	6564.084799	8.370138	-0.049709	4.376157
243.819481	6572.082204	8.375142	-0.049754	4.378732
243.876212	6580.096734	8.380147	-0.049770	4.381310
243.926421	6588.073378	8.385152	-0.049784	4.383874
244.208627	6596.144256	8.390157	-0.049842	4.386469
244.477017	6604.127854	8.395162	-0.049898	4.389033
244.716528	6612.174118	8.400166	-0.049948	4.391617
244.826776	6620.212649	8.405171	-0.049974	4.394195
245.029848	6628.265231	8.410176	-0.050017	4.396777
245.454584	6636.220769	8.415181	-0.050101	4.399327
245.563357	6644.231730	8.420186	-0.050127	4.401892
245.454000	6652.213581	8.425190	-0.050112	4.404446
245.768781	6660.296328	8.430195	-0.050176	4.407032
245.902054	6668.276166	8.435200	-0.050206	4.409582
246.128515	6676.353221	8.440205	-0.050253	4.412163
246.297856	6684.327309	8.445210	-0.050290	4.414709
246.708136	6692.408445	8.450214	-0.050372	4.417289
246.677373	6700.345774	8.455219	-0.050371	4.419819
246.817175	6708.391186	8.460224	-0.050403	4.422383
247.090510	6716.376784	8.465229	-0.050459	4.424927
247.104051	6724.448034	8.470234	-0.050467	4.427496
247.457015	6732.407656	8.475238	-0.050538	4.430029
247.629006	6740.493163	8.480243	-0.050575	4.432600
247.704188	6748.475549	8.485248	-0.050595	4.435136
248.025337	6756.557852	8.490253	-0.050660	4.437704
248.052338	6764.473383	8.495258	-0.050670	4.440216
248.147680	6772.534388	8.500262	-0.050693	4.442773
248.389046	6780.529396	8.505267	-0.050744	4.445308
248.409833	6788.588805	8.510272	-0.050753	4.447861
248.778253	6796.556181	8.515277	-0.050827	4.450385
248.912472	6804.595008	8.520282	-0.050857	4.452929
248.880937	6812.625504	8.525286	-0.050857	4.455468
249.183835	6820.667834	8.530291	-0.050918	4.458011
249.413570	6828.617783	8.535296	-0.050966	4.460523
249.410327	6836.663768	8.540301	-0.050971	4.463063
249.673563	6844.630460	8.545306	-0.051026	4.465578
249.992679	6852.657644	8.550310	-0.051090	4.468110
249.972758	6860.715638	8.555315	-0.051092	4.470650
250.094467	6868.728268	8.560320	-0.051120	4.473174
250.460068	6876.760045	8.565325	-0.051193	4.475703
250.653879	6884.779247	8.570330	-0.051235	4.478227
250.844566	6892.747467	8.575335	-0.051276	4.480733
250.844970	6900.769612	8.580339	-0.051281	4.483254
251.010274	6908.737187	8.585344	-0.051317	4.485757
251.368941	6916.819076	8.590349	-0.051389	4.488294
251.380787	6924.798059	8.595354	-0.051397	4.490798
251.695260	6932.916516	8.600359	-0.051461	4.493344
251.788779	6940.891964	8.605363	-0.051483	4.495843
251.727095	6948.876075	8.610368	-0.051477	4.498344
252.022507	6956.893872	8.615373	-0.051538	4.500854
252.351496	6964.907043	8.620378	-0.051604	4.503362
252.612822	6972.910315	8.625383	-0.051658	4.505865
252.739229	6980.943060	8.630387	-0.051687	4.508375
252.899744	6988.954116	8.635392	-0.051722	4.510877
253.361437	6997.046779	8.640397	-0.051814	4.513404
253.382211	7005.049836	8.645402	-0.051823	4.515901
253.568407	7013.066347	8.650407	-0.051863	4.518401
253.655887	7021.000773	8.655411	-0.051885	4.520873
253.763379	7029.003645	8.660416	-0.051910	4.523366
253.947584	7037.027615	8.665421	-0.051950	4.525864
253.993351	7045.015676	8.670426	-0.051963	4.528349
254.148143	7053.059823	8.675431	-0.051998	4.530850
254.590888	7061.102046	8.680435	-0.052085	4.533350
254.550188	7069.093856	8.685440	-0.052083	4.535832
254.678843	7077.135549	8.690445	-0.052112	4.538329
254.783457	7085.107342	8.695450	-0.052137	4.540802
255.423675	7093.144775	8.700455	-0.052262	4.543295
255.481195	7101.150877	8.705459	-0.052278	4.545776
255.291636	7109.165330	8.710464	-0.052248	4.548258
255.536435	7117.235019	8.715469	-0.052299	4.550756
255.830579	7125.270726	8.720474	-0.052359	4.553242
255.937715	7133.247909	8.725479	-0.052384	4.555709
255.963066	7141.283263	8.730483	-0.052394	4.558192
256.333703	7149.231073	8.735488	-0.052469	4.560647
256.595589	7157.314095	8.740493	-0.052523	4.563143
256.708128	7165.274471	8.745498	-0.052549	4.565599
256.796908	7173.346586	8.750503	-0.052571	4.568088
256.990142	7181.320600	8.755507	-0.052612	4.570546
257.048211	7189.394529	8.760512	-0.052628	4.573033
257.382968	7197.428832	8.765517	-0.052696	4.575506
257.451156	7205.433480	8.770522	-0.052714	4.577969
257.360963	7213.404070	8.775527	-0.052703	4.580420
257.505879	7221.463004	8.780531	-0.052735	4.582897
257.766871	7229.397165	8.785536	-0.052789	4.585335
258.023862	7237.523832	8.790541	-0.052842	4.587830
257.958300	7245.455688	8.795546	-0.052835	4.590264
258.354796	7253.545402	8.800551	-0.052914	4.592745
258.578013	7261.583620	8.805555	-0.052961	4.595209
258.576920	7269.584409	8.810560	-0.052966	4.597660
258.895760	7277.525349	8.815565	-0.053031	4.600091
258.952154	7285.561286	8.820570	-0.053047	4.602550
259.195917	7293.530230	8.825575	-0.053098	4.604988
259.170981	7301.628884	8.830579	-0.053098	4.607463
259.284647	7309.559323	8.835584	-0.053125	4.609886
259.642654	7317.642606	8.840589	-0.053197	4.612355
259.730536	7325.649110	8.845594	-0.053219	4.614798
259.873952	7333.687639	8.850599	-0.053251	4.617250
259.950393	7341.654576	8.855603	-0.053270	4.619679
259.938354	7349.683968	8.860608	-0.053273	4.622126
260.391474	7357.651042	8.865613	-0.053363	4.624552
260.438981	7365.703520	8.870618	-0.053377	4.627003
260.727041	7373.726058	8.875623	-0.053436	4.629444
260.870990	7381.784363	8.880627	-0.053468	4.631894
261.008460	7389.762718	8.885632	-0.053499	4.634318
261.294782	7397.787963	8.890637	-0.053558	4.636756
261.264191	7405.773225	8.895642	-0.053558	4.639180
261.639988	7413.818727	8.900647	-0.053633	4.641621
261.812288	7421.800884	8.905651	-0.053670	4.644041
261.918555	7429.794221	8.910656	-0.053695	4.646464
262.013988	7437.851519	8.915661	-0.053719	4.648905
262.079323	7445.877895	8.920666	-0.053736	4.651335
262.349179	7453.891925	8.925671	-0.053792	4.653760
262.480282	7461.930215	8.930675	-0.053821	4.656191
262.565564	7469.901255	8.935680	-0.053843	4.658600
262.812002	7477.951732	8.940685	-0.053894	4.661032
263.023566	7485.936010	8.945690	-0.053939	4.663443
263.093185	7493.906111	8.950695	-0.053957	4.665849
263.202900	7501.962374	8.955699	-0.053983	4.668279
263.446171	7509.959487	8.960704	-0.054033	4.670690
263.542013	7518.094619	8.965709	-0.054056	4.673141
263.779891	7526.128201	8.970714	-0.054106	4.675560
264.222258	7534.106209	8.975719	-0.054194	4.677961
264.521425	7542.061563	8.980723	-0.054255	4.680354
264.593268	7550.010157	8.985728	-0.054273	4.682744
264.806834	7558.051150	8.990733	-0.054319	4.685161
264.811740	7566.059485	8.995738	-0.054325	4.687567
264.978070	7574.055500	9.000743	-0.054361	4.689967
265.262623	7582.129456	9.005747	-0.054420	4.692389
265.416886	7590.145226	9.010752	-0.054454	4.694793
265.609904	7598.173827	9.015757	-0.054495	4.697200
265.580698	7606.115120	9.020762	-0.054495	4.699579
266.121349	7614.179022	9.025767	-0.054601	4.701993
266.087690	7622.157698	9.030771	-0.054600	4.704381
266.273133	7630.187290	9.035776	-0.054640	4.706783
266.522931	7638.258211	9.040781	-0.054692	4.709196
266.584871	7646.236518	9.045786	-0.054708	4.711580
266.733165	7654.251093	9.050791	-0.054741	4.713974
267.038183	7662.353979	9.055795	-0.054804	4.716392
267.279704	7670.304586	9.060800	-0.054854	4.718764
267.194581	7678.286318	9.065805	-0.054843	4.721145
267.482057	7686.326220	9.070810	-0.054902	4.723540
267.571139	7694.311619	9.075815	-0.054924	4.725919
267.706887	7702.400161	9.080819	-0.054955	4.728328
267.780885	7710.339030	9.085824	-0.054974	4.730691
267.916973	7718.412762	9.090829	-0.055005	4.733092
268.061209	7726.426684	9.095834	-0.055037	4.735474
268.260919	7734.496837	9.100839	-0.055079	4.737872
268.443390	7742.424830	9.105843	-0.055119	4.740226
268.444247	7750.467209	9.110848	-0.055124	4.742614
268.644802	7758.452943	9.115853	-0.055167	4.744983
268.678539	7766.524918	9.120858	-0.055178	4.747377
269.150114	7774.533813	9.125863	-0.055272	4.749749
269.226046	7782.556601	9.130867	-0.055291	4.752126
269.312251	7790.578303	9.135872	-0.055312	4.754501
269.615166	7798.593199	9.140877	-0.055374	4.756873
269.740026	7806.573949	9.145882	-0.055403	4.759233
269.792152	7814.549282	9.150887	-0.055418	4.761591
269.972594	7822.585306	9.155891	-0.055457	4.763965
270.064804	7830.568157	9.160896	-0.055479	4.766323
270.529765	7838.587779	9.165901	-0.055571	4.768689
270.565311	7846.637156	9.170906	-0.055583	4.771064
270.542642	7854.642075	9.175911	-0.055584	4.773425
270.678014	7862.703074	9.180915	-0.055615	4.775801
270.805810	7870.675831	9.185920	-0.055644	4.778150
271.369025	7878.722780	9.190925	-0.055754	4.780517
271.419486	7886.732132	9.195930	-0.055769	4.782875
271.491330	7894.657701	9.200935	-0.055788	4.785206
271.799819	7902.734250	9.205939	-0.055850	4.787580
271.865151	7910.694194	9.210944	-0.055868	4.789919
272.099101	7918.846800	9.215949	-0.055917	4.792313
272.105383	7926.791420	9.220954	-0.055923	4.794646
272.220501	7934.838542	9.225959	-0.055950	4.797007
272.525379	7942.771494	9.230963	-0.056012	4.799333
272.460605	7950.815067	9.235968	-0.056005	4.801691
272.773103	7958.809357	9.240973	-0.056069	4.804033
272.786850	7966.873938	9.245978	-0.056077	4.806395
273.051005	7974.847682	9.250983	-0.056131	4.808728
273.230673	7982.910354	9.255987	-0.056170	4.811086
273.175980	7990.424075	9.260992	-0.056165	4.813284
273.547640	7995.130263	9.265997	-0.056237	4.814658

273.501084	7997.751548	9.271002	-0.056231	4.815424
273.553756	7999.051440	9.276007	-0.056241	4.815804
273.708326	7999.666363	9.281011	-0.056271	4.815983
273.631304	7999.622249	9.286016	-0.056256	4.815971
273.900124	8000.050174	9.291021	-0.056307	4.816094
274.130681	8000.018040	9.296026	-0.056350	4.816084
273.992007	8000.110619	9.301031	-0.056324	4.816111
274.134745	8000.079031	9.306035	-0.056351	4.816101
274.236254	8000.210149	9.311040	-0.056370	4.816139
274.496428	8000.084539	9.316045	-0.056418	4.816101
274.231763	8000.170562	9.321050	-0.056369	4.816128
274.369486	8000.194436	9.326055	-0.056395	4.816134
274.394904	8000.066708	9.331059	-0.056400	4.816096
274.378012	8000.298242	9.336064	-0.056397	4.816164
274.400899	8000.002740	9.341069	-0.056401	4.816078
274.558133	8000.238498	9.346074	-0.056431	4.816146
274.652508	8000.281885	9.351079	-0.056448	4.816158
274.781915	8000.062027	9.356083	-0.056473	4.816093
274.894572	8000.017073	9.361088	-0.056494	4.816079
274.916015	7999.864702	9.366093	-0.056498	4.816035
274.859641	8000.089110	9.371098	-0.056487	4.816100
274.694771	8000.196172	9.376103	-0.056457	4.816133
274.853934	8000.127489	9.381107	-0.056487	4.816112
274.907907	8000.239587	9.386112	-0.056497	4.816144
274.977918	7999.975918	9.391117	-0.056510	4.816067
274.928834	8000.138496	9.396122	-0.056501	4.816114
275.042830	8000.055106	9.401127	-0.056522	4.816089
275.218097	8000.018766	9.406131	-0.056555	4.816078
275.222566	8000.090437	9.411136	-0.056556	4.816099
275.314654	7999.993830	9.416141	-0.056573	4.816070
275.375768	8000.146655	9.421146	-0.056585	4.816114
275.299715	8000.177338	9.426151	-0.056571	4.816124
275.411313	8000.083221	9.431155	-0.056591	4.816096
275.460911	8000.120455	9.436160	-0.056601	4.816106
275.403985	8000.083111	9.441165	-0.056590	4.816096
275.338876	8000.183435	9.446170	-0.056578	4.816125
275.419752	8000.124017	9.451175	-0.056594	4.816108
275.405186	8000.057526	9.456179	-0.056591	4.816088
275.380711	8000.105169	9.461184	-0.056586	4.816102
275.616373	7999.984456	9.466189	-0.056630	4.816066
275.474645	8000.148561	9.471194	-0.056604	4.816114
275.716942	8000.025831	9.476199	-0.056649	4.816077
275.786438	8000.014282	9.481203	-0.056662	4.816074
275.817339	8000.086433	9.486208	-0.056668	4.816094
275.767056	7999.955193	9.491213	-0.056659	4.816056
275.892074	8000.150845	9.496218	-0.056683	4.816113
276.006000	8000.364462	9.501223	-0.056704	4.816175
275.991820	8000.128104	9.506227	-0.056701	4.816106
275.895241	8000.237475	9.511232	-0.056684	4.816138
275.981356	7999.983707	9.516237	-0.056700	4.816064
275.855717	8000.176952	9.521242	-0.056676	4.816121
275.755751	8000.176219	9.526247	-0.056658	4.816121
275.996681	7999.927396	9.531251	-0.056703	4.816047
275.931224	8000.328996	9.536256	-0.056691	4.816165
276.054658	8000.041716	9.541261	-0.056714	4.816080
276.092794	8000.292419	9.546266	-0.056721	4.816153
276.068699	7999.984302	9.551271	-0.056717	4.816063
276.001789	7999.888016	9.556275	-0.056704	4.816035
275.907815	8000.375637	9.561280	-0.056687	4.816178
276.204742	7999.959025	9.566285	-0.056742	4.816055
276.011082	8000.162788	9.571290	-0.056706	4.816116
275.866458	8000.226416	9.576295	-0.056680	4.816135
276.079949	8000.025172	9.581299	-0.056719	4.816075
275.968072	8000.381061	9.586304	-0.056699	4.816180
276.076091	8000.074269	9.591309	-0.056719	4.816089
276.118829	8000.102833	9.596314	-0.056727	4.816098
276.180455	8000.101826	9.601319	-0.056739	4.816097
276.163940	8000.217991	9.606323	-0.056736	4.816131
276.082835	8000.382131	9.611328	-0.056721	4.816179
276.202370	8000.146060	9.616333	-0.056743	4.816110
276.151204	8000.169717	9.621338	-0.056734	4.816117
276.150369	8000.005183	9.626343	-0.056734	4.816069
276.214499	8000.007426	9.631347	-0.056746	4.816069
276.263685	8000.162175	9.636352	-0.056755	4.816114
276.244067	7999.870165	9.641357	-0.056751	4.816029
276.277842	7999.929549	9.646362	-0.056758	4.816046
276.224540	8000.002311	9.651367	-0.056748	4.816068
276.229071	7999.876338	9.656371	-0.056749	4.816031
276.175141	8000.248233	9.661376	-0.056739	4.816140
276.361979	7999.997359	9.666381	-0.056774	4.816065
276.444749	8000.100367	9.671386	-0.056790	4.816095
276.406644	8000.000328	9.676391	-0.056782	4.816066
276.200192	8000.078861	9.681395	-0.056744	4.816090
276.152409	8000.116467	9.686400	-0.056735	4.816101
276.329438	7999.928450	9.691405	-0.056768	4.816045
276.384725	8000.114292	9.696410	-0.056779	4.816099
276.458505	7999.859232	9.701415	-0.056793	4.816025
276.541856	7999.983617	9.706419	-0.056808	4.816060
276.593363	8000.014477	9.711424	-0.056818	4.816069
276.771084	7999.860660	9.716429	-0.056851	4.816023
276.522340	8000.106161	9.721434	-0.056805	4.816096
276.396030	7999.959651	9.726439	-0.056782	4.816054
276.704866	7999.890476	9.731443	-0.056839	4.816032
276.705182	8000.138358	9.736448	-0.056840	4.816105
276.609193	7999.989191	9.741453	-0.056822	4.816062
276.420824	8000.185574	9.746458	-0.056787	4.816120
276.636807	7999.886082	9.751463	-0.056827	4.816031
276.774029	7999.813796	9.756467	-0.056853	4.816010
276.543750	8000.075657	9.761472	-0.056810	4.816087
276.474306	7999.820136	9.766477	-0.056797	4.816013
276.608081	7999.961461	9.771482	-0.056822	4.816054
276.596147	8000.026427	9.776487	-0.056820	4.816073
276.664812	8000.012727	9.781491	-0.056833	4.816068
276.419304	7999.969824	9.786496	-0.056787	4.816057
276.514824	7999.858320	9.791501	-0.056805	4.816024
276.529574	8000.084026	9.796506	-0.056808	4.816090
276.548106	8000.134588	9.801511	-0.056812	4.816104
276.576469	7999.996224	9.806515	-0.056817	4.816064
276.380833	8000.135850	9.811520	-0.056781	4.816106
276.594800	7999.963459	9.816525	-0.056821	4.816054
276.776062	8000.025519	9.821530	-0.056855	4.816071
276.738002	8000.024840	9.826535	-0.056848	4.816071
276.885037	8000.120468	9.831539	-0.056875	4.816099
276.862253	7999.969423	9.836544	-0.056871	4.816054
276.863094	7999.834834	9.841549	-0.056871	4.816015
276.752545	8000.013397	9.846554	-0.056851	4.816068
276.756373	7999.991042	9.851559	-0.056852	4.816061
276.725723	7999.864428	9.856563	-0.056846	4.816025
276.736284	7999.894546	9.861568	-0.056848	4.816033
276.761256	7999.819155	9.866573	-0.056853	4.816011
276.773300	7999.919812	9.871578	-0.056855	4.816040
276.697610	7999.988964	9.876583	-0.056841	4.816061
276.797958	7999.852974	9.881587	-0.056860	4.816021
276.789561	8000.000270	9.886592	-0.056859	4.816064
276.989755	7999.870364	9.891597	-0.056896	4.816025
277.047916	7999.961175	9.896602	-0.056907	4.816051
277.083656	8000.065468	9.901607	-0.056914	4.816081
277.029963	7999.838007	9.906611	-0.056904	4.816015
276.967504	8000.281338	9.911616	-0.056893	4.816145
277.060696	7999.862092	9.916621	-0.056910	4.816022
276.933747	7999.935656	9.921626	-0.056886	4.816044
276.989045	8000.125776	9.926631	-0.056897	4.816099
276.973270	7999.918233	9.931635	-0.056894	4.816039
276.817179	7999.957080	9.936640	-0.056865	4.816051
276.939933	7999.767010	9.941645	-0.056888	4.815995
276.986155	7999.997561	9.946650	-0.056897	4.816062
277.025577	7999.918159	9.951655	-0.056904	4.816039
276.977896	7999.926921	9.956659	-0.056895	4.816041
276.750068	8000.132204	9.961664	-0.056853	4.816103
276.879172	7999.849298	9.966669	-0.056877	4.816019
276.990665	8000.076761	9.971674	-0.056898	4.816085
276.839413	7999.983216	9.976679	-0.056870	4.816059
276.935693	7999.953990	9.981683	-0.056888	4.816049
276.989026	8000.084244	9.986688	-0.056898	4.816087
277.128280	7999.940411	9.991693	-0.056924	4.816045
276.904209	8000.067770	9.996698	-0.056883	4.816083
277.025226	7999.864846	10.001703	-0.056905	4.816023
277.088824	7999.846780	10.006707	-0.056917	4.816017
276.887080	8000.047194	10.011712	-0.056880	4.816077
277.041419	7999.867311	10.016717	-0.056908	4.816024
277.048810	7999.889892	10.021722	-0.056910	4.816030
277.132816	7999.976898	10.026727	-0.056926	4.816055
277.122764	7999.953223	10.031731	-0.056924	4.816048
277.075970	8000.194911	10.036736	-0.056916	4.816119
277.293498	7999.932838	10.041741	-0.056956	4.816041
277.320833	8000.020953	10.046746	-0.056961	4.816067
277.324639	8000.117190	10.051751	-0.056962	4.816095
277.171452	7999.940273	10.056755	-0.056934	4.816044
277.236439	8000.154075	10.061760	-0.056946	4.816106
277.395946	7999.837529	10.066765	-0.056976	4.816013
277.184764	8000.017473	10.071770	-0.056937	4.816067
277.002012	8000.008828	10.076775	-0.056903	4.816065
277.234586	7999.872030	10.081779	-0.056946	4.816024
277.335275	8000.012759	10.086784	-0.056965	4.816064
277.404415	7999.870859	10.091789	-0.056978	4.816023
277.094205	7999.930416	10.096794	-0.056920	4.816042
277.188656	8000.004791	10.101799	-0.056938	4.816063
277.510414	7999.881363	10.106803	-0.056998	4.816025
277.310366	8000.068989	10.111808	-0.056961	4.816081
277.360113	7999.839129	10.116813	-0.056970	4.816014
277.339350	7999.926372	10.121818	-0.056966	4.816039
277.485894	7999.997419	10.126823	-0.056994	4.816059
277.447606	8000.061908	10.131827	-0.056987	4.816078
277.119646	7999.833745	10.136832	-0.056926	4.816013
277.347505	8000.003490	10.141837	-0.056968	4.816062
277.347086	8000.049435	10.146842	-0.056969	4.816075
277.279035	8000.189241	10.151847	-0.056956	4.816116
277.425896	7999.870328	10.156851	-0.056983	4.816022
277.235308	8000.027141	10.161856	-0.056948	4.816069
277.201073	7999.869478	10.166861	-0.056942	4.816023
277.160574	8000.168974	10.171866	-0.056934	4.816111
277.313041	7999.842685	10.176871	-0.056963	4.816015
277.285363	7999.944760	10.181875	-0.056958	4.816045
277.159080	7999.910429	10.186880	-0.056934	4.816035
277.329736	7999.874005	10.191885	-0.056966	4.816024
277.385834	7999.895333	10.196890	-0.056977	4.816030
277.309598	7999.911056	10.201895	-0.056963	4.816035
277.508442	7999.942453	10.206899	-0.057000	4.816043
277.469092	8000.168252	10.211904	-0.056993	4.816109
277.316675	7999.778738	10.216909	-0.056964	4.815996
277.346981	7999.931011	10.221914	-0.056970	4.816040
277.318711	7999.895252	10.226919	-0.056965	4.816030
277.420432	7999.838347	10.231923	-0.056984	4.816013
277.352135	8000.168324	10.236928	-0.056972	4.816110
277.637726	7999.824148	10.241933	-0.057025	4.816008
277.395763	8000.011014	10.246938	-0.056980	4.816064
277.338950	8000.001447	10.251943	-0.056969	4.816061
277.449559	7999.778034	10.256947	-0.056990	4.815995
277.406702	7999.860602	10.261952	-0.056982	4.816020
277.447426	7999.850668	10.266957	-0.056990	4.816016
277.385034	7999.990576	10.271962	-0.056978	4.816058
277.205919	7999.855926	10.276967	-0.056945	4.816019
277.420182	7999.995510	10.281971	-0.056985	4.816059
277.182305	8000.122619	10.286976	-0.056941	4.816097
277.172833	7999.858565	10.291981	-0.056939	4.816020
277.221166	7999.875479	10.296986	-0.056948	4.816025
277.226805	7999.777301	10.301991	-0.056950	4.815996
277.188023	7999.885584	10.306995	-0.056943	4.816028
277.463309	7999.873495	10.312000	-0.056994	4.816023
277.504412	7999.957587	10.317005	-0.057002	4.816047
277.427416	8000.003211	10.322010	-0.056988	4.816061
277.451674	8000.034646	10.327015	-0.056992	4.816070
277.419085	7999.878080	10.332019	-0.056986	4.816025
277.196474	8000.015081	10.337024	-0.056945	4.816066
277.420754	7999.859970	10.342029	-0.056987	4.816019
277.509958	7999.921430	10.347034	-0.057003	4.816037
277.432165	8000.000160	10.352039	-0.056989	4.816060
277.634516	7999.972858	10.357043	-0.057027	4.816051
277.684469	7999.871209	10.362048	-0.057036	4.816021
277.768729	8000.005232	10.367053	-0.057052	4.816060
277.474233	8000.013789	10.372058	-0.056997	4.816064
277.558332	7999.946948	10.377063	-0.057013	4.816044
277.659481	7999.799219	10.382067	-0.057032	4.816000
277.449403	8000.075340	10.387072	-0.056993	4.816082
277.601384	7999.872975	10.392077	-0.057021	4.816022
277.778316	7999.832392	10.397082	-0.057055	4.816009
277.539238	7999.876144	10.402087	-0.057010	4.816023
277.861151	7999.955715	10.407091	-0.057070	4.816045
277.748535	7999.938726	10.412096	-0.057049	4.816040
277.811354	7999.828763	10.417101	-0.057061	4.816008
277.681849	8000.003780	10.422106	-0.057037	4.816060
277.774855	7999.959537	10.427111	-0.057055	4.816046
277.692159	7999.807404	10.432115	-0.057039	4.816002
277.496298	7999.854077	10.437120	-0.057003	4.816017
277.796171	7999.868075	10.442125	-0.057059	4.816020
277.785308	8000.016398	10.447130	-0.057057	4.816063
277.669170	7999.927761	10.452135	-0.057036	4.816038
277.534208	7999.895409	10.457139	-0.057010	4.816029
277.679102	7999.846766	10.462144	-0.057038	4.816014
277.688911	7999.971958	10.467149	-0.057040	4.816050
277.648883	8000.024663	10.472154	-0.057032	4.816066
277.776951	7999.895584	10.477159	-0.057056	4.816028
277.910194	7999.867029	10.482163	-0.057081	4.816019
277.735661	8000.077556	10.487168	-0.057049	4.816081
277.733382	7999.846750	10.492173	-0.057048	4.816014
277.746712	7999.864097	10.497178	-0.057051	4.816019
277.786412	8000.176805	10.502183	-0.057059	4.816110
277.842786	7999.790006	10.507187	-0.057069	4.815996
277.535309	8000.026967	10.512192	-0.057012	4.816067
277.641140	7999.933810	10.517197	-0.057032	4.816040
277.444096	7999.981530	10.522202	-0.056995	4.816054
277.671588	8000.113878	10.527207	-0.057038	4.816092
277.742056	7999.824561	10.532211	-0.057051	4.816007
277.556824	7999.881043	10.537216	-0.057017	4.816025
277.682227	7999.899355	10.542221	-0.057040	4.816029
277.999955	7999.909405	10.547226	-0.057099	4.816030
277.806699	7999.930483	10.552231	-0.057063	4.816038
277.848557	7999.881039	10.557235	-0.057071	4.816023
277.942027	7999.876335	10.562240	-0.057089	4.816021
277.971674	7999.857653	10.567245	-0.057094	4.816015
277.665266	7999.796549	10.572250	-0.057038	4.815999
277.589367	7999.828304	10.577255	-0.057024	4.816009
277.769298	7999.911710	10.582259	-0.057057	4.816032
277.869672	7999.790675	10.587264	-0.057076	4.815996
277.876262	7999.839953	10.592269	-0.057077	4.816011
277.776610	7999.899055	10.597274	-0.057059	4.816029
277.711792	7999.848744	10.602279	-0.057047	4.816014
277.619658	7999.818238	10.607283	-0.057030	4.816006
277.668324	7999.867210	10.612288	-0.057039	4.816020
277.749245	7999.787491	10.617293	-0.057054	4.815996
277.755967	7999.933995	10.622298	-0.057056	4.816039
277.721624	7999.971846	10.627303	-0.057049	4.816050
277.831025	7999.988800	10.632307	-0.057070	4.816054
277.695198	7999.859207	10.637312	-0.057045	4.816017
277.866091	8000.002280	10.642317	-0.057077	4.816058
278.052304	7999.989644	10.647322	-0.057111	4.816054
277.732286	7999.977438	10.652327	-0.057052	4.816052
277.721560	7999.929176	10.657331	-0.057050	4.816038
277.748138	7999.851677	10.662336	-0.057055	4.816015
277.875585	7999.832632	10.667341	-0.057079	4.816009
277.717600	7999.881060	10.672346	-0.057050	4.816024
277.769032	7999.993119	10.677351	-0.057059	4.816056
277.993694	7999.826261	10.682355	-0.057101	4.816006
277.858628	7999.846259	10.687360	-0.057076	4.816013
277.920052	7999.850590	10.692365	-0.057088	4.816014
277.740852	7999.912523	10.697370	-0.057055	4.816033
277.725901	7999.828927	10.702375	-0.057052	4.816008
277.703390	7999.854172	10.707379	-0.057048	4.816016
277.737401	7999.943478	10.712384	-0.057054	4.816042
277.932361	7999.872238	10.717389	-0.057091	4.816020
277.921078	8000.013075	10.722394	-0.057089	4.816061
277.863553	7999.862465	10.727399	-0.057078	4.816017
278.012781	7999.982709	10.732403	-0.057106	4.816052
277.919319	7999.979956	10.737408	-0.057089	4.816051
277.825254	7999.939798	10.742413	-0.057071	4.816040
277.821702	7999.967523	10.747418	-0.057071	4.816048
277.892864	7999.981647	10.752423	-0.057084	4.816052
277.910898	7999.890102	10.757427	-0.057088	4.816025
277.699693	8000.039064	10.762432	-0.057049	4.816070
277.789237	7999.965911	10.767437	-0.057065	4.816048
277.877591	7999.843590	10.772442	-0.057082	4.816012
277.819745	8000.001745	10.777447	-0.057071	4.816058
277.989582	7999.870218	10.782451	-0.057103	4.816019
278.061301	7999.912130	10.787456	-0.057116	4.816031
278.090783	7999.746005	10.792461	-0.057122	4.815982
278.190836	7999.881382	10.797466	-0.057141	4.816021
278.023223	8000.158279	10.802471	-0.057110	4.816103
278.125505	7999.858851	10.807475	-0.057129	4.816015
278.037926	7999.994031	10.812480	-0.057113	4.816055
278.125044	7999.805445	10.817485	-0.057129	4.815999
278.039393	7999.906470	10.822490	-0.057113	4.816029
277.811388	7999.870293	10.827495	-0.057071	4.816020
277.958868	7999.786439	10.832499	-0.057098	4.815995
277.879949	7999.992289	10.837504	-0.057084	4.816055
277.786516	7999.831413	10.842509	-0.057066	4.816009
277.902818	7999.897638	10.847514	-0.057088	4.816027
277.951218	7999.872886	10.852519	-0.057097	4.816020
278.005640	7999.879227	10.857523	-0.057108	4.816021
277.817874	8000.000835	10.862528	-0.057073	4.816058
278.130493	7999.868694	10.867533	-0.057131	4.816018
278.222653	7999.841530	10.872538	-0.057148	4.816009
278.122987	7999.979696	10.877543	-0.057130	4.816050
278.172202	7999.804311	10.882547	-0.057139	4.815999
277.920595	7999.909804	10.887552	-0.057092	4.816031
278.024659	7999.872172	10.892557	-0.057112	4.816019
277.907654	7999.926687	10.897562	-0.057090	4.816036
277.999515	8000.119612	10.902567	-0.057108	4.816092
278.026949	7999.872248	10.907571	-0.057113	4.816019
277.827799	7999.900698	10.912576	-0.057076	4.816029
277.870989	7999.852347	10.917581	-0.057084	4.816014
277.864410	7999.869333	10.922586	-0.057083	4.816019
277.864459	7999.998623	10.927591	-0.057083	4.816057
278.057876	7999.881413	10.932595	-0.057119	4.816022
277.926972	7999.865160	10.937600	-0.057095	4.816018
278.079971	7999.835895	10.942605	-0.057123	4.816008
277.914925	7999.895948	10.947610	-0.057093	4.816027
277.984260	7999.885465	10.952615	-0.057106	4.816023
278.145819	7999.903365	10.957619	-0.057136	4.816028
277.973036	7999.830795	10.962624	-0.057104	4.816007
277.915486	7999.859678	10.967629	-0.057093	4.816016
278.164913	8000.087514	10.972634	-0.057140	4.816081
278.111303	7999.873937	10.977639	-0.057130	4.816019
278.163864	7999.827892	10.982643	-0.057140	4.816005
278.013252	7999.850813	10.987648	-0.057112	4.816013
278.094784	7999.813840	10.992653	-0.057127	4.816002
278.161140	7999.890913	10.997658	-0.057140	4.816024
278.057641	7999.859131	11.002663	-0.057121	4.816015
277.912511	7999.865056	11.007667	-0.057094	4.816018
277.918087	7999.859827	11.012672	-0.057095	4.816016
277.900251	7999.874472	11.017677	-0.057092	4.816020
278.043128	7999.945454	11.022682	-0.057118	4.816040
277.937069	8000.001236	11.027687	-0.057099	4.816057
278.149789	7999.877965	11.032691	-0.057138	4.816020
278.083561	8000.013532	11.037696	-0.057126	4.816060
278.176626	7999.907322	11.042701	-0.057144	4.816029
277.973553	7999.970959	11.047706	-0.057106	4.816048
278.023162	7999.975076	11.052711	-0.057115	4.816049
278.276985	7999.852551	11.057715	-0.057163	4.816012
278.070354	8000.079592	11.062720	-0.057125	4.816079
278.225797	7999.861261	11.067725	-0.057153	4.816015
278.031961	7999.898355	11.072730	-0.057117	4.816027
277.958995	7999.840417	11.077735	-0.057104	4.816010
278.005243	7999.816694	11.082739	-0.057113	4.816003
278.039940	7999.987212	11.087744	-0.057119	4.816053
278.141437	7999.949534	11.092749	-0.057138	4.816041
278.044606	8000.040741	11.097754	-0.057121	4.816068
278.216869	8000.166748	11.102759	-0.057153	4.816104
278.414379	7999.867979	11.107763	-0.057189	4.816016
278.235546	7999.847650	11.112768	-0.057156	4.816011
278.078737	8000.076663	11.117773	-0.057127	4.816079
278.484081	7999.859662	11.122778	-0.057203	4.816013
278.240168	7999.959952	11.127783	-0.057158	4.816044
278.278553	7999.862365	11.132787	-0.057165	4.816015
278.254435	8000.182467	11.137792	-0.057161	4.816109
278.357159	7999.906551	11.142797	-0.057180	4.816027
278.312422	7999.934598	11.147802	-0.057171	4.816036
278.167693	7999.856126	11.152807	-0.057145	4.816014
278.313582	7999.814979	11.157811	-0.057172	4.816001
278.066316	7999.960082	11.162816	-0.057126	4.816045
278.058420	7999.994140	11.167821	-0.057125	4.816054
278.173400	7999.876574	11.172826	-0.057146	4.816020
278.130105	7999.934563	11.177831	-0.057138	4.816037
278.198290	7999.795849	11.182835	-0.057151	4.815996
278.325543	8000.086644	11.187840	-0.057175	4.816080
278.170256	7999.835963	11.192845	-0.057146	4.816008
278.202150	8000.096180	11.197850	-0.057152	4.816084
278.167573	7999.848758	11.202855	-0.057146	4.816011
278.343660	7999.847691	11.207859	-0.057179	4.816010
278.256657	7999.893134	11.212864	-0.057163	4.816024
278.121890	7999.872537	11.217869	-0.057138	4.816019
278.244378	7999.885455	11.222874	-0.057161	4.816022
278.131643	8000.044752	11.227879	-0.057140	4.816069
278.246852	7999.936806	11.232883	-0.057161	4.816037
278.161526	7999.989759	11.237888	-0.057146	4.816053
278.219716	7999.862616	11.242893	-0.057156	4.816015
278.145142	7999.942474	11.247898	-0.057143	4.816039
278.193036	7999.874975	11.252903	-0.057152	4.816019
278.212321	7999.897773	11.257907	-0.057155	4.816025
278.167412	7999.900175	11.262912	-0.057147	4.816026
278.336879	7999.851977	11.267917	-0.057179	4.816011
278.365051	7999.850363	11.272922	-0.057184	4.816011
278.220592	7999.941774	11.277927	-0.057157	4.816038
278.248903	7999.840799	11.282931	-0.057163	4.816009
278.368431	7999.995764	11.287936	-0.057185	4.816053
278.324547	7999.832579	11.292941	-0.057177	4.816006
278.282274	7999.898065	11.297946	-0.057169	4.816025
278.416337	7999.867388	11.302951	-0.057194	4.816015
278.464026	7999.806296	11.307955	-0.057203	4.815997
278.361668	7999.852529	11.312960	-0.057184	4.816011
278.363723	8000.000020	11.317965	-0.057185	4.816054
278.402243	8000.006073	11.322970	-0.057192	4.816056
278.343847	7999.842624	11.327975	-0.057181	4.816009
278.260545	7999.848603	11.332979	-0.057166	4.816011
278.136175	8000.038673	11.337984	-0.057143	4.816067
278.164052	7999.949443	11.342989	-0.057148	4.816041
278.289567	7999.868395	11.347994	-0.057172	4.816016
278.127219	7999.965892	11.352999	-0.057142	4.816046
278.406730	7999.764770	11.358003	-0.057194	4.815985
278.341449	8000.033908	11.363008	-0.057182	4.816064
278.299874	7999.951964	11.368013	-0.057174	4.816041
278.424990	7999.977752	11.373018	-0.057198	4.816048
278.333219	7999.873529	11.378023	-0.057181	4.816018
278.471193	7999.945491	11.383027	-0.057207	4.816038
278.357087	7999.845137	11.388032	-0.057185	4.816009
278.345891	7999.938967	11.393037	-0.057183	4.816037
278.172827	7999.789464	11.398042	-0.057151	4.815994
278.055864	7999.959368	11.403047	-0.057130	4.816044
278.235673	7999.867553	11.408051	-0.057163	4.816016
278.302943	8000.050417	11.413056	-0.057176	4.816069
278.212123	7999.921638	11.418061	-0.057159	4.816032
278.080593	7999.814558	11.423066	-0.057135	4.816002
278.190368	7999.851819	11.428071	-0.057155	4.816012
278.297748	7999.824931	11.433075	-0.057175	4.816004
278.203946	7999.889482	11.438080	-0.057158	4.816023
278.303392	7999.973567	11.443085	-0.057177	4.816047
278.417782	7999.942533	11.448090	-0.057198	4.816037
278.351684	7999.913566	11.453095	-0.057186	4.816029
278.396764	7999.774432	11.458099	-0.057194	4.815988
278.334963	8000.037222	11.463104	-0.057183	4.816065
278.207504	7999.769953	11.468109	-0.057159	4.815988
278.427924	7999.954526	11.473114	-0.057201	4.816041
278.383254	7999.753932	11.478119	-0.057192	4.815982
278.517744	7999.893142	11.483123	-0.057217	4.816022
278.268592	7999.911069	11.488128	-0.057171	4.816029
278.245273	7999.882878	11.493133	-0.057167	4.816021
278.386970	7999.796782	11.498138	-0.057193	4.815995
278.227257	7999.867616	11.503143	-0.057164	4.816016
278.258910	7999.837218	11.508147	-0.057170	4.816007
278.371230	7999.851019	11.513152	-0.057191	4.816011
278.304118	7999.849813	11.518157	-0.057178	4.816011
278.255512	7999.868174	11.523162	-0.057170	4.816016
278.043929	7999.990419	11.528167	-0.057130	4.816053
278.411812	7999.862485	11.533171	-0.057199	4.816014
278.202206	8000.011478	11.538176	-0.057160	4.816059
278.426112	7999.851015	11.543181	-0.057202	4.816010
278.227478	7999.829259	11.548186	-0.057165	4.816005
278.278191	7999.869722	11.553191	-0.057174	4.816017
278.440400	7999.813914	11.558195	-0.057205	4.816000
278.404290	7999.765191	11.563200	-0.057198	4.815985
278.368532	7999.825453	11.568205	-0.057192	4.816003
278.347425	7999.853929	11.573210	-0.057188	4.816012
278.434230	8000.039285	11.578215	-0.057204	4.816065
278.556991	7999.854549	11.583219	-0.057227	4.816011
278.539349	7999.985657	11.588224	-0.057224	4.816049
278.395447	7999.768304	11.593229	-0.057197	4.815986
278.289826	7999.871104	11.598234	-0.057178	4.816017
278.300230	7999.946093	11.603239	-0.057180	4.816039
278.416636	7999.840306	11.608243	-0.057202	4.816007
278.316180	7999.972048	11.613248	-0.057183	4.816046
278.508706	7999.809947	11.618253	-0.057219	4.815998
278.728366	7999.859887	11.623258	-0.057260	4.816011
278.504324	7999.926348	11.628263	-0.057218	4.816032
278.620304	7999.845127	11.633267	-0.057240	4.816008
278.408980	7999.990883	11.638272	-0.057201	4.816051
278.271137	7999.943519	11.643277	-0.057175	4.816038
278.383445	7999.908174	11.648282	-0.057196	4.816027
278.329234	8000.008702	11.653287	-0.057186	4.816057
278.208743	7999.816348	11.658291	-0.057164	4.816001
278.521086	7999.912842	11.663296	-0.057222	4.816028
278.448068	7999.757676	11.668301	-0.057209	4.815983
278.339420	7999.894610	11.673306	-0.057189	4.816024
278.327362	7999.912566	11.678311	-0.057187	4.816029
278.413957	7999.888507	11.683315	-0.057203	4.816021
278.354453	7999.966502	11.688320	-0.057192	4.816045
278.339697	7999.961972	11.693325	-0.057189	4.816043
278.566942	7999.910549	11.698330	-0.057232	4.816027
278.554132	8000.135768	11.703335	-0.057230	4.816093
278.646977	7999.957967	11.708339	-0.057247	4.816040
278.511750	8000.016424	11.713344	-0.057222	4.816058
278.526921	7999.897047	11.718349	-0.057225	4.816023
278.488284	7999.881399	11.723354	-0.057218	4.816019
278.373704	8000.028911	11.728359	-0.057196	4.816063
278.578715	7999.877721	11.733363	-0.057235	4.816017
278.559468	7999.891272	11.738368	-0.057231	4.816021
278.463278	7999.874580	11.743373	-0.057213	4.816017
278.686170	7999.898936	11.748378	-0.057255	4.816023
278.569726	7999.912861	11.753383	-0.057233	4.816028
278.394957	7999.906495	11.758387	-0.057201	4.816027
278.420978	7999.875995	11.763392	-0.057206	4.816018
278.645409	7999.962348	11.768397	-0.057248	4.816042
278.481331	7999.760655	11.773402	-0.057217	4.815984
278.386010	8000.139296	11.778407	-0.057200	4.816095
278.682843	7999.749376	11.783411	-0.057255	4.815979
278.531562	8000.000927	11.788416	-0.057227	4.816054
278.513156	7999.833930	11.793421	-0.057224	4.816005
278.484868	7999.923176	11.798426	-0.057219	4.816031
278.496177	7999.851808	11.803431	-0.057221	4.816010
278.585758	7999.775450	11.808435	-0.057238	4.815987
278.505451	8000.003716	11.813440	-0.057223	4.816054
278.700088	7999.755110	11.818445	-0.057259	4.815981
278.621262	7999.881902	11.823450	-0.057245	4.816018
278.398849	7999.992199	11.828455	-0.057203	4.816052
278.494800	7999.862535	11.833459	-0.057221	4.816013
278.420701	7999.911418	11.838464	-0.057208	4.816028
278.552436	7999.887109	11.843469	-0.057232	4.816020
278.680097	7999.911874	11.848474	-0.057256	4.816027
278.725682	7999.815486	11.853479	-0.057265	4.815998
278.566321	7999.860684	11.858483	-0.057235	4.816012
278.432826	7999.925584	11.863488	-0.057211	4.816032
278.743245	7999.800881	11.868493	-0.057268	4.815994
278.607517	7999.845440	11.873498	-0.057243	4.816008
278.422834	7999.857057	11.878503	-0.057209	4.816012
278.619178	7999.786911	11.883507	-0.057246	4.815990
278.571317	8000.101241	11.888512	-0.057237	4.816083
278.678861	7999.825411	11.893517	-0.057257	4.816001
278.599606	7999.947922	11.898522	-0.057242	4.816038
278.772821	7999.853850	11.903527	-0.057275	4.816009
278.637691	7999.802261	11.908531	-0.057250	4.815995
278.557975	7999.929037	11.913536	-0.057235	4.816032
278.364618	7999.941566	11.918541	-0.057199	4.816037
278.642815	7999.861152	11.923546	-0.057251	4.816012
278.421644	7999.878518	11.928551	-0.057210	4.816018
278.511596	7999.883367	11.933555	-0.057227	4.816019
278.612217	7999.863836	11.938560	-0.057246	4.816013
278.589976	7999.789722	11.943565	-0.057242	4.815991
278.596316	7999.888144	11.948570	-0.057243	4.816020
278.720563	7999.952379	11.953575	-0.057266	4.816038
278.581126	7999.866522	11.958579	-0.057240	4.816014
278.405222	7999.869752	11.963584	-0.057208	4.816016
278.526666	7999.866625	11.968589	-0.057230	4.816014
278.681279	7999.855552	11.973594	-0.057259	4.816010
278.471638	7999.857101	11.978599	-0.057220	4.816012
278.454281	7999.884577	11.983603	-0.057217	4.816020
278.650970	7999.910595	11.988608	-0.057254	4.816026
278.743155	7999.793683	11.993613	-0.057271	4.815992
278.466668	7999.821799	11.998618	-0.057220	4.816001
278.755094	7999.850550	12.003623	-0.057274	4.816008
278.915429	7999.866292	12.008627	-0.057304	4.816012
278.508059	7999.885621	12.013632	-0.057228	4.816020
278.598576	7999.833854	12.018637	-0.057245	4.816004
278.753354	7999.925354	12.023642	-0.057274	4.816030
278.704082	7999.894555	12.028647	-0.057265	4.816021
278.686211	7999.806630	12.033651	-0.057262	4.815996
278.801031	7999.802315	12.038656	-0.057283	4.815994
278.706144	7999.885010	12.043661	-0.057266	4.816019
278.655112	7999.840290	12.048666	-0.057256	4.816006
278.640753	7999.827219	12.053671	-0.057254	4.816002
278.913576	7999.859961	12.058675	-0.057305	4.816010
278.755487	7999.870993	12.063680	-0.057275	4.816014
278.793506	7999.840710	12.068685	-0.057282	4.816005
278.762451	7999.829473	12.073690	-0.057277	4.816002
278.802697	7999.866542	12.078695	-0.057284	4.816013
278.846539	7999.849185	12.083699	-0.057293	4.816007
278.755154	7999.874249	12.088704	-0.057276	4.816015
278.729986	7999.850298	12.093709	-0.057271	4.816008
278.700852	7999.822001	12.098714	-0.057266	4.816000
278.703753	8000.034684	12.103719	-0.057267	4.816062
278.880202	7999.810321	12.108723	-0.057299	4.815996
278.603232	7999.856590	12.113728	-0.057248	4.816011
278.625514	7999.831364	12.118733	-0.057252	4.816003
278.694789	7999.965118	12.123738	-0.057265	4.816042
278.471654	7999.907658	12.128743	-0.057224	4.816026
278.595597	7999.863976	12.133747	-0.057247	4.816013
278.707850	7999.852135	12.138752	-0.057268	4.816009
278.808674	7999.887098	12.143757	-0.057287	4.816019
278.843212	7999.952911	12.148762	-0.057294	4.816038
278.703378	7999.980300	12.153767	-0.057268	4.816046
278.580299	7999.854140	12.158771	-0.057245	4.816010
278.672309	7999.959459	12.163776	-0.057262	4.816040
278.543503	7999.844947	12.168781	-0.057238	4.816008
278.694943	7999.864802	12.173786	-0.057267	4.816013
278.627539	7999.909532	12.178791	-0.057254	4.816026
278.696402	7999.846687	12.183795	-0.057267	4.816007
278.681687	7999.793010	12.188800	-0.057264	4.815992
278.972826	7999.869890	12.193805	-0.057319	4.816013
278.826742	7999.901440	12.198810	-0.057292	4.816023
278.590620	7999.871524	12.203815	-0.057248	4.816015
278.753578	7999.766581	12.208819	-0.057278	4.815984
278.726308	7999.894309	12.213824	-0.057273	4.816021
278.848440	7999.761915	12.218829	-0.057296	4.815982
278.860532	7999.945916	12.223834	-0.057299	4.816035
278.886646	7999.813915	12.228839	-0.057303	4.815997
278.753189	7999.815778	12.233843	-0.057279	4.815998
278.720080	7999.927374	12.238848	-0.057273	4.816031
278.567638	7999.769697	12.243853	-0.057244	4.815985
278.661909	7999.857962	12.248858	-0.057262	4.816011
278.782335	7999.876185	12.253863	-0.057285	4.816015
278.987574	7999.831842	12.258867	-0.057323	4.816001
278.945895	7999.839644	12.263872	-0.057315	4.816004
278.946176	7999.925136	12.268877	-0.057316	4.816029
279.132386	7999.846257	12.273882	-0.057350	4.816005
278.926869	7999.859633	12.278887	-0.057312	4.816010
278.925525	7999.750640	12.283891	-0.057312	4.815978
279.020713	7999.868838	12.288896	-0.057330	4.816012
278.853743	7999.902146	12.293901	-0.057299	4.816023
278.840779	7999.759820	12.298906	-0.057297	4.815981
278.848227	7999.908479	12.303911	-0.057298	4.816025
279.035264	7999.825342	12.308915	-0.057333	4.815999
278.906971	7999.915979	12.313920	-0.057309	4.816026
278.827786	7999.793820	12.318925	-0.057295	4.815991
278.875655	7999.868422	12.323930	-0.057304	4.816013
278.868279	7999.873641	12.328935	-0.057302	4.816014
278.910302	7999.769709	12.333939	-0.057310	4.815984
278.722352	7999.861400	12.338944	-0.057275	4.816011
278.740211	7999.887377	12.343949	-0.057279	4.816019
278.774933	7999.983110	12.348954	-0.057286	4.816047
278.692854	7999.849145	12.353959	-0.057270	4.816008
278.850315	7999.772951	12.358963	-0.057300	4.815985
278.768455	8000.033243	12.363968	-0.057285	4.816061
278.663783	7999.737536	12.368973	-0.057265	4.815976
278.819254	7999.908112	12.373978	-0.057294	4.816025
278.781179	7999.971538	12.378983	-0.057287	4.816043
278.852665	7999.765571	12.383987	-0.057301	4.815983
278.748635	7999.900454	12.388992	-0.057282	4.816023
278.828879	7999.849568	12.393997	-0.057297	4.816007
278.922079	7999.861955	12.399002	-0.057314	4.816010
278.878443	7999.875064	12.404007	-0.057306	4.816015
278.871168	7999.866396	12.409011	-0.057305	4.816012
278.949197	7999.902014	12.414016	-0.057319	4.816022
278.873372	7999.875006	12.419021	-0.057305	4.816015
279.008981	7999.844357	12.424026	-0.057331	4.816005
278.879970	7999.766169	12.429031	-0.057307	4.815983
278.836420	7999.934202	12.434035	-0.057299	4.816032
278.791227	7999.845781	12.439040	-0.057291	4.816006
278.845005	7999.774116	12.444045	-0.057301	4.815985
278.775019	7999.905342	12.449050	-0.057288	4.816024
278.705518	7999.740623	12.454055	-0.057275	4.815976
278.773043	7999.873276	12.459059	-0.057288	4.816015
278.854095	7999.853390	12.464064	-0.057303	4.816008
278.823853	7999.931917	12.469069	-0.057297	4.816031
278.749185	7999.911341	12.474074	-0.057284	4.816026
278.808909	7999.772471	12.479079	-0.057295	4.815985
278.839069	7999.854231	12.484083	-0.057301	4.816009
278.797339	8000.034051	12.489088	-0.057293	4.816061
278.878896	7999.757749	12.494093	-0.057308	4.815980
278.973212	7999.967818	12.499098	-0.057326	4.816041
278.746011	7999.873956	12.504103	-0.057284	4.816015
279.009449	7999.774042	12.509107	-0.057333	4.815984
279.114247	7999.908442	12.514112	-0.057353	4.816023
279.061588	7999.872239	12.519117	-0.057343	4.816013
279.019841	7999.869356	12.524122	-0.057335	4.816012
279.037453	7999.883576	12.529127	-0.057339	4.816016
279.040724	7999.818472	12.534131	-0.057339	4.815997
278.989592	7999.937221	12.539136	-0.057330	4.816032
278.963732	7999.886546	12.544141	-0.057325	4.816017
279.019909	7999.855524	12.549146	-0.057336	4.816008
279.028490	7999.994589	12.554151	-0.057338	4.816049
278.808442	7999.796150	12.559155	-0.057297	4.815992
278.909531	7999.874923	12.564160	-0.057316	4.816014
278.805006	7999.881585	12.569165	-0.057296	4.816017
278.844432	7999.898338	12.574170	-0.057304	4.816021
278.913142	7999.811985	12.579175	-0.057317	4.815996
278.756501	7999.843343	12.584179	-0.057288	4.816006
278.847366	7999.886673	12.589184	-0.057305	4.816018
278.784202	7999.827842	12.594189	-0.057293	4.816001
278.855794	7999.883643	12.599194	-0.057306	4.816017
278.670546	7999.869608	12.604199	-0.057272	4.816014
278.920668	7999.801505	12.609203	-0.057319	4.815993
278.992702	7999.933174	12.614208	-0.057332	4.816031
278.791002	7999.821612	12.619213	-0.057295	4.815999
278.755311	7999.825249	12.624218	-0.057288	4.816000
278.836697	7999.785069	12.629223	-0.057303	4.815988
279.062722	7999.835125	12.634227	-0.057346	4.816002
279.009610	7999.905758	12.639232	-0.057336	4.816023
278.726330	7999.823700	12.644237	-0.057283	4.816000
278.968664	7999.869779	12.649242	-0.057329	4.816012
278.898798	7999.892028	12.654247	-0.057316	4.816019
279.060544	7999.826595	12.659251	-0.057346	4.815999
278.779334	7999.834323	12.664256	-0.057294	4.816003
278.910579	7999.845264	12.669261	-0.057318	4.816005
278.986209	7999.832758	12.674266	-0.057332	4.816001
278.893896	7999.883448	12.679271	-0.057315	4.816017
279.151315	7999.803725	12.684275	-0.057363	4.815992
279.035096	7999.948003	12.689280	-0.057342	4.816035
278.999221	7999.787097	12.694285	-0.057335	4.815988
279.057658	7999.851207	12.699290	-0.057346	4.816006
279.071613	7999.772407	12.704295	-0.057349	4.815983
279.094940	7999.927766	12.709299	-0.057353	4.816029
279.113816	7999.865082	12.714304	-0.057357	4.816010
279.070382	7999.820499	12.719309	-0.057349	4.815997
279.115691	7999.840564	12.724314	-0.057358	4.816003
278.967145	7999.789800	12.729319	-0.057330	4.815989
278.973099	7999.856162	12.734323	-0.057331	4.816008
278.834983	7999.916705	12.739328	-0.057306	4.816027
278.735121	7999.863618	12.744333	-0.057287	4.816012
278.986366	7999.774168	12.749338	-0.057334	4.815984
279.148441	7999.854048	12.754343	-0.057364	4.816007
279.035698	7999.903298	12.759347	-0.057344	4.816022
279.133236	7999.806783	12.764352	-0.057362	4.815993
279.194745	7999.823938	12.769357	-0.057373	4.815998
278.905938	7999.831528	12.774362	-0.057320	4.816001
279.065020	7999.995762	12.779367	-0.057350	4.816049
279.166019	7999.853367	12.784371	-0.057368	4.816006
278.909774	7999.831632	12.789376	-0.057321	4.816001
279.030391	7999.787890	12.794381	-0.057343	4.815988
279.146633	7999.818859	12.799386	-0.057365	4.815996
278.994087	7999.952862	12.804391	-0.057337	4.816036
278.971288	7999.806083	12.809395	-0.057333	4.815994
279.058014	7999.856817	12.814400	-0.057349	4.816008
279.145133	7999.907558	12.819405	-0.057365	4.816022
279.069065	7999.890162	12.824410	-0.057351	4.816018
278.832599	7999.808953	12.829415	-0.057307	4.815995
279.174548	7999.875004	12.834419	-0.057371	4.816013
279.171543	7999.784143	12.839424	-0.057371	4.815986
278.949616	7999.979925	12.844429	-0.057330	4.816045
279.157741	7999.874733	12.849434	-0.057368	4.816013
279.019812	7999.926731	12.854439	-0.057343	4.816029
279.144908	7999.830717	12.859443	-0.057366	4.816000
279.021600	7999.822079	12.864448	-0.057343	4.815998
278.887668	7999.899792	12.869453	-0.057319	4.816021
278.976565	7999.854406	12.874458	-0.057335	4.816008
279.044751	7999.790480	12.879463	-0.057348	4.815989
279.050960	7999.844026	12.884467	-0.057349	4.816004
278.818420	7999.958413	12.889472	-0.057306	4.816039
278.879682	7999.791792	12.894477	-0.057318	4.815990
279.054054	7999.808858	12.899482	-0.057350	4.815994
278.917548	7999.985890	12.904487	-0.057325	4.816046
278.933954	7999.857986	12.909491	-0.057328	4.816009
279.080293	7999.987798	12.914496	-0.057356	4.816046
279.114909	7999.791844	12.919501	-0.057362	4.815989
279.174634	7999.854909	12.924506	-0.057373	4.816007
278.904625	7999.873525	12.929511	-0.057323	4.816014
279.179630	7999.814422	12.934515	-0.057374	4.815995
279.179076	7999.786644	12.939520	-0.057374	4.815987
279.180581	7999.911690	12.944525	-0.057375	4.816023
279.144953	7999.852290	12.949530	-0.057368	4.816006
279.056053	7999.923342	12.954535	-0.057352	4.816027
279.132876	7999.801877	12.959539	-0.057366	4.815991
279.110512	7999.807893	12.964544	-0.057362	4.815993
279.174353	7999.869965	12.969549	-0.057374	4.816011
278.949949	7999.770812	12.974554	-0.057333	4.815983
279.018828	7999.972940	12.979559	-0.057346	4.816042
278.958953	7999.752834	12.984563	-0.057334	4.815978
278.829677	7999.907560	12.989568	-0.057311	4.816024
278.737285	7999.905894	12.994573	-0.057294	4.816024
278.941199	7999.850842	12.999578	-0.057332	4.816007
279.094996	7999.885699	13.004583	-0.057360	4.816016
279.113506	7999.793091	13.009587	-0.057364	4.815989
279.083466	7999.873759	13.014592	-0.057358	4.816013
279.145358	7999.886647	13.019597	-0.057370	4.816016
279.152719	7999.850465	13.024602	-0.057372	4.816005
278.980868	7999.818509	13.029607	-0.057340	4.815997
279.210568	7999.821621	13.034611	-0.057383	4.815997
278.986490	7999.868850	13.039616	-0.057341	4.816012
279.008596	7999.804088	13.044621	-0.057345	4.815993
279.166296	7999.868931	13.049626	-0.057375	4.816011
279.027619	7999.895273	13.054631	-0.057349	4.816019
278.976475	7999.770418	13.059635	-0.057339	4.815983
279.059781	7999.907633	13.064640	-0.057355	4.816023
279.113431	7999.902207	13.069645	-0.057365	4.816021
279.212324	7999.830291	13.074650	-0.057384	4.815999
278.904580	7999.858907	13.079655	-0.057327	4.816009
279.077763	7999.864198	13.084659	-0.057359	4.816010
279.258198	7999.885649	13.089664	-0.057393	4.816015
279.267030	7999.825987	13.094669	-0.057394	4.815998
279.097350	7999.944721	13.099674	-0.057363	4.816033
279.133894	7999.804361	13.104679	-0.057370	4.815992
279.117911	7999.776303	13.109683	-0.057367	4.815984
279.076868	7999.849292	13.114688	-0.057360	4.816005
279.128015	7999.885490	13.119693	-0.057369	4.816016
279.263587	7999.828130	13.124698	-0.057394	4.815998
279.099936	7999.908509	13.129703	-0.057364	4.816023
279.338738	7999.833790	13.134707	-0.057409	4.816000
279.305733	7999.788328	13.139712	-0.057403	4.815986
279.204573	7999.941428	13.144717	-0.057384	4.816032
279.285083	7999.814687	13.149722	-0.057399	4.815994
279.222069	7999.795391	13.154727	-0.057387	4.815989
279.251697	7999.894237	13.159731	-0.057393	4.816018
279.116695	7999.858676	13.164736	-0.057368	4.816008
279.138393	7999.887929	13.169741	-0.057372	4.816016
279.289877	7999.820173	13.174746	-0.057401	4.815996
279.165899	7999.823276	13.179751	-0.057378	4.815997
279.318641	7999.807896	13.184755	-0.057406	4.815992
279.486671	7999.982979	13.189760	-0.057438	4.816042
279.272127	7999.850881	13.194765	-0.057398	4.816005
279.405547	7999.906737	13.199770	-0.057423	4.816020
279.260080	7999.896628	13.204775	-0.057396	4.816018
279.223648	7999.820119	13.209779	-0.057389	4.815996
279.356439	7999.898400	13.214784	-0.057414	4.816018
279.227443	7999.800978	13.219789	-0.057390	4.815990
279.286861	7999.876859	13.224794	-0.057401	4.816012
279.055163	7999.937840	13.229799	-0.057358	4.816031
278.894580	7999.807792	13.234803	-0.057328	4.815994
279.242502	7999.821597	13.239808	-0.057393	4.815996
279.013543	7999.863396	13.244813	-0.057351	4.816010
279.074346	7999.865579	13.249818	-0.057362	4.816010
279.172493	7999.811813	13.254823	-0.057381	4.815994
279.232237	7999.899453	13.259827	-0.057392	4.816019
279.158347	7999.858590	13.264832	-0.057378	4.816008
279.191011	7999.883769	13.269837	-0.057384	4.816015
279.228176	7999.835307	13.274842	-0.057391	4.816000
279.147719	7999.829584	13.279847	-0.057377	4.815999
279.218349	7999.943064	13.284851	-0.057390	4.816032
279.076176	7999.860361	13.289856	-0.057363	4.816009
279.158939	7999.905681	13.294861	-0.057379	4.816021
279.332042	7999.798785	13.299866	-0.057411	4.815989
279.318432	7999.878682	13.304871	-0.057409	4.816013
279.359339	7999.779002	13.309875	-0.057417	4.815983
279.333996	7999.820223	13.314880	-0.057412	4.815995
279.285948	7999.918728	13.319885	-0.057403	4.816025
279.470368	7999.812037	13.324890	-0.057438	4.815992
279.364077	7999.814392	13.329895	-0.057418	4.815994
279.317320	7999.895826	13.334899	-0.057409	4.816018
279.257476	7999.824233	13.339904	-0.057398	4.815997
279.290506	7999.879335	13.344909	-0.057405	4.816013
279.458022	7999.826828	13.349914	-0.057436	4.815997
279.369283	7999.851939	13.354919	-0.057420	4.816005
279.316804	7999.824287	13.359923	-0.057410	4.815997
279.147543	7999.905633	13.364928	-0.057379	4.816021
279.199790	7999.807227	13.369933	-0.057388	4.815992
279.279941	7999.835405	13.374938	-0.057403	4.816000
279.221635	7999.930518	13.379943	-0.057393	4.816028
279.266360	7999.758253	13.384947	-0.057401	4.815978
279.340272	7999.922010	13.389952	-0.057415	4.816025
279.379545	7999.818026	13.394957	-0.057422	4.815995
279.459224	7999.906029	13.399962	-0.057437	4.816020
279.290020	7999.941432	13.404967	-0.057406	4.816031
279.382669	7999.796748	13.409971	-0.057423	4.815988
279.419862	7999.950223	13.414976	-0.057430	4.816033
279.354830	7999.781307	13.419981	-0.057418	4.815984
279.448300	7999.821479	13.424986	-0.057436	4.815995
279.338341	7999.846206	13.429991	-0.057416	4.816003
279.551799	7999.849024	13.434995	-0.057455	4.816003
279.330022	7999.957196	13.440000	-0.057414	4.816035
279.353861	7999.831563	13.445005	-0.057419	4.815999
279.346889	7999.841064	13.450010	-0.057418	4.816001
279.228255	7999.791910	13.455015	-0.057396	4.815988
279.253292	7999.907768	13.460019	-0.057400	4.816021
279.386397	7999.896306	13.465024	-0.057425	4.816017
279.332133	7999.914565	13.470029	-0.057415	4.816023
279.399720	7999.857038	13.475034	-0.057428	4.816006
279.438251	7999.852407	13.480039	-0.057435	4.816004
279.382460	7999.842858	13.485043	-0.057425	4.816002
279.263535	7999.884516	13.490048	-0.057403	4.816015
279.381165	7999.870636	13.495053	-0.057425	4.816010
279.430101	7999.902521	13.500058	-0.057434	4.816019
279.337181	7999.871998	13.505063	-0.057417	4.816010
279.451930	7999.932857	13.510067	-0.057439	4.816028
279.515528	7999.877395	13.515072	-0.057451	4.816011
279.286745	7999.831583	13.520077	-0.057408	4.815999
279.376959	7999.888792	13.525082	-0.057425	4.816015
279.386232	7999.845165	13.530087	-0.057427	4.816002
279.331998	7999.907230	13.535091	-0.057417	4.816021
279.524476	7999.863724	13.540096	-0.057453	4.816007
279.538472	7999.788130	13.545101	-0.057455	4.815985
279.460032	7999.932027	13.550106	-0.057441	4.816027
279.368898	7999.870550	13.555111	-0.057424	4.816010
279.353075	7999.901259	13.560115	-0.057421	4.816019
279.481978	7999.870489	13.565120	-0.057445	4.816009
279.190304	7999.821399	13.570125	-0.057391	4.815996
279.381075	7999.801367	13.575130	-0.057427	4.815990
279.412515	7999.891699	13.580135	-0.057433	4.816016
279.446968	7999.869898	13.585139	-0.057439	4.816009
279.540759	7999.907940	13.590144	-0.057457	4.816020
279.327024	7999.844238	13.595149	-0.057417	4.816002
279.599047	7999.843845	13.600154	-0.057468	4.816001
279.348011	7999.838231	13.605159	-0.057421	4.816000
279.545464	7999.982863	13.610163	-0.057458	4.816042
279.552361	7999.907139	13.615168	-0.057460	4.816020
279.212073	7999.869987	13.620173	-0.057396	4.816010
279.325176	7999.922269	13.625178	-0.057418	4.816025
279.343521	7999.846753	13.630183	-0.057421	4.816003
279.361918	7999.831072	13.635187	-0.057425	4.815998
279.316924	7999.902921	13.640192	-0.057416	4.816020
279.233143	7999.806320	13.645197	-0.057401	4.815992
279.165215	7999.873479	13.650202	-0.057388	4.816012
279.125512	7999.908028	13.655207	-0.057381	4.816022
279.217967	7999.788983	13.660211	-0.057398	4.815987
279.291397	7999.873666	13.665216	-0.057412	4.816011
279.260062	7999.837850	13.670221	-0.057407	4.816001
279.459201	7999.844682	13.675226	-0.057444	4.816002
279.402059	7999.921653	13.680231	-0.057433	4.816025
279.311108	7999.822784	13.685235	-0.057416	4.815996
279.350833	7999.911130	13.690240	-0.057424	4.816022
279.270132	7999.802831	13.695245	-0.057409	4.815990
279.343206	7999.899261	13.700250	-0.057423	4.816018
279.165851	7999.875752	13.705255	-0.057390	4.816012
279.344250	7999.812758	13.710259	-0.057423	4.815993
279.548540	7999.927597	13.715264	-0.057461	4.816025
279.422971	7999.801388	13.720269	-0.057438	4.815989
279.237877	7999.863215	13.725274	-0.057404	4.816008
279.452806	7999.939783	13.730279	-0.057444	4.816030
279.488343	7999.854963	13.735283	-0.057451	4.816005
279.373460	7999.872121	13.740288	-0.057429	4.816010
279.311755	7999.778057	13.745293	-0.057418	4.815983
279.444984	7999.910838	13.750298	-0.057443	4.816021
279.337503	7999.789232	13.755303	-0.057423	4.815986
279.367120	7999.756659	13.760307	-0.057429	4.815976
279.439352	7999.936413	13.765312	-0.057442	4.816029
279.353689	7999.816271	13.770317	-0.057426	4.815994
279.262289	7999.912920	13.775322	-0.057409	4.816023
279.386955	7999.820103	13.780327	-0.057433	4.815995
279.553012	7999.817786	13.785331	-0.057464	4.815993
279.519173	7999.838552	13.790336	-0.057458	4.816000
279.365541	7999.833638	13.795341	-0.057429	4.815999
279.406299	7999.903839	13.800346	-0.057437	4.816019
279.146503	7999.848916	13.805351	-0.057389	4.816005
279.455283	7999.900477	13.810355	-0.057446	4.816018
279.471682	7999.879417	13.815360	-0.057449	4.816012
279.261398	7999.802956	13.820365	-0.057410	4.815990
279.269253	7999.805247	13.825370	-0.057412	4.815991
279.445924	7999.854409	13.830375	-0.057445	4.816005
279.313320	7999.941763	13.835379	-0.057420	4.816031
279.336511	7999.896252	13.840384	-0.057425	4.816017
279.492422	7999.768742	13.845389	-0.057454	4.815979
279.571671	7999.867422	13.850394	-0.057469	4.816008
279.688434	7999.877032	13.855399	-0.057491	4.816010
279.444868	7999.892922	13.860403	-0.057445	4.816016
279.505012	7999.836329	13.865408	-0.057457	4.815999
279.273969	7999.889842	13.870413	-0.057414	4.816016
279.436493	7999.789164	13.875418	-0.057444	4.815985
279.321385	7999.975133	13.880423	-0.057423	4.816040
279.552046	7999.793421	13.885427	-0.057466	4.815986
279.386966	7999.937882	13.890432	-0.057435	4.816029
279.400622	7999.765052	13.895437	-0.057438	4.815979
279.592614	7999.905311	13.900442	-0.057474	4.816019
279.584268	7999.850680	13.905447	-0.057472	4.816003
279.597861	7999.912909	13.910451	-0.057475	4.816021
279.660085	7999.890544	13.915456	-0.057487	4.816014
279.619016	7999.806470	13.920461	-0.057479	4.815990
279.549842	7999.877880	13.925466	-0.057466	4.816011
279.380859	7999.835291	13.930471	-0.057435	4.815999
279.663940	7999.916302	13.935475	-0.057488	4.816021
279.549168	7999.819137	13.940480	-0.057467	4.815994
279.510057	7999.879340	13.945485	-0.057460	4.816011
279.620289	7999.816177	13.950490	-0.057480	4.815992
279.485062	7999.882114	13.955495	-0.057455	4.816012
279.334917	7999.808882	13.960499	-0.057427	4.815992
279.405113	7999.859316	13.965504	-0.057440	4.816006
279.371016	7999.849093	13.970509	-0.057434	4.816003
279.675373	7999.794796	13.975514	-0.057491	4.815986
279.439528	7999.910193	13.980519	-0.057447	4.816021
279.535161	7999.863860	13.985523	-0.057465	4.816007
279.712224	7999.875634	13.990528	-0.057498	4.816009
279.599825	7999.886426	13.995533	-0.057477	4.816013
279.488939	7999.854507	14.000538	-0.057457	4.816004
279.620274	7999.914600	14.005543	-0.057481	4.816021
279.306400	7999.890748	14.010547	-0.057423	4.816016
279.421864	7999.956964	14.015552	-0.057445	4.816035
279.482797	7999.854441	14.020557	-0.057456	4.816004
279.411928	7999.856371	14.025562	-0.057443	4.816005
279.339509	7999.911696	14.030567	-0.057430	4.816022
279.558768	7999.874018	14.035571	-0.057471	4.816010
279.612845	7999.866463	14.040576	-0.057481	4.816007
279.453150	7999.812290	14.045581	-0.057451	4.815992
279.365575	7999.871613	14.050586	-0.057435	4.816010
279.425494	7999.849206	14.055591	-0.057446	4.816003
279.372367	7999.819405	14.060595	-0.057437	4.815995
279.436882	7999.846230	14.065600	-0.057449	4.816002
279.438106	7999.856948	14.070605	-0.057449	4.816005
279.591790	7999.856544	14.075610	-0.057478	4.816004
279.639697	7999.942903	14.080615	-0.057487	4.816029
279.661245	7999.865307	14.085619	-0.057491	4.816006
279.626591	7999.789898	14.090624	-0.057485	4.815985
279.502763	7999.892369	14.095629	-0.057462	4.816015
279.624215	7999.909544	14.100634	-0.057484	4.816020
279.508560	7999.832664	14.105639	-0.057463	4.815998
279.445026	7999.931957	14.110643	-0.057451	4.816027
279.529776	7999.881152	14.115648	-0.057467	4.816012
279.479395	7999.822552	14.120653	-0.057458	4.815995
279.660209	7999.810888	14.125658	-0.057492	4.815990
279.582745	7999.870395	14.130663	-0.057477	4.816008
279.630977	7999.863803	14.135667	-0.057486	4.816006
279.884931	7999.898343	14.140672	-0.057534	4.816015
279.669198	7999.896573	14.145677	-0.057494	4.816015
279.536291	7999.905925	14.150682	-0.057469	4.816019
279.604848	7999.840936	14.155687	-0.057482	4.816000
279.576013	7999.846835	14.160691	-0.057477	4.816001
279.543484	7999.934938	14.165696	-0.057471	4.816027
279.457723	7999.857531	14.170701	-0.057455	4.816005
279.616427	7999.860424	14.175706	-0.057485	4.816005
279.682682	7999.771888	14.180711	-0.057497	4.815979
279.565744	7999.874485	14.185715	-0.057475	4.816010
279.690200	7999.916289	14.190720	-0.057499	4.816021
279.660074	7999.864467	14.195725	-0.057493	4.816006
279.604429	7999.873084	14.200730	-0.057483	4.816009
279.617478	7999.910729	14.205735	-0.057486	4.816020
279.630236	7999.867165	14.210739	-0.057488	4.816007
279.640898	7999.943231	14.215744	-0.057490	4.816029
279.599470	7999.864492	14.220749	-0.057483	4.816006
279.578606	7999.920753	14.225754	-0.057479	4.816023
279.496622	7999.864784	14.230759	-0.057464	4.816007
279.539936	7999.870925	14.235763	-0.057472	4.816009
279.738735	7999.907668	14.240768	-0.057509	4.816018
279.606494	7999.853992	14.245773	-0.057484	4.816003
279.732987	7999.883011	14.250778	-0.057508	4.816011
279.720903	7999.893488	14.255783	-0.057506	4.816014
279.583621	7999.910239	14.260787	-0.057481	4.816020
279.639184	7999.882411	14.265792	-0.057491	4.816011
279.504484	7999.618206	14.270797	-0.057466	4.815935

279.447967	7996.365183	14.275802	-0.057453	4.814985
279.488515	7990.791784	14.280807	-0.057457	4.813355
279.414584	7983.995984	14.285811	-0.057439	4.811368
279.425581	7976.663565	14.290816	-0.057437	4.809223
279.282649	7969.012871	14.295821	-0.057405	4.806985
279.292785	7961.192556	14.300826	-0.057402	4.804695
279.359966	7953.391861	14.305831	-0.057410	4.802409
279.424065	7945.386087	14.310835	-0.057416	4.800062
279.231692	7937.474678	14.315840	-0.057376	4.797743
279.197016	7929.403804	14.320845	-0.057364	4.795376
279.380307	7921.423419	14.325850	-0.057393	4.793032
279.200626	7913.381534	14.330855	-0.057354	4.790671
279.021056	7905.405304	14.335859	-0.057316	4.788329
279.495799	7897.441176	14.340864	-0.057399	4.785985
278.994199	7889.405189	14.345869	-0.057301	4.783624
279.049411	7881.408388	14.350874	-0.057306	4.781271
278.954805	7873.416435	14.355879	-0.057283	4.778918
278.988077	7865.385857	14.360883	-0.057284	4.776553
278.828315	7857.461276	14.365888	-0.057250	4.774218
278.517515	7849.365899	14.370893	-0.057186	4.771833
278.895679	7841.390348	14.375898	-0.057252	4.769478
278.850779	7833.366105	14.380903	-0.057238	4.767110
278.839757	7825.355859	14.385907	-0.057231	4.764745
278.849817	7817.444978	14.390912	-0.057228	4.762408
278.517718	7809.334839	14.395917	-0.057161	4.760012
278.446151	7801.444532	14.400922	-0.057143	4.757679
278.468200	7793.349429	14.405927	-0.057142	4.755284
278.458232	7785.314927	14.410931	-0.057135	4.752905
278.442201	7777.343399	14.415936	-0.057127	4.750545
278.410163	7769.334567	14.420941	-0.057116	4.748172
278.379926	7761.327677	14.425946	-0.057105	4.745798
278.231119	7753.349681	14.430951	-0.057072	4.743432
278.288394	7745.369777	14.435955	-0.057078	4.741064
278.473226	7737.398500	14.440960	-0.057107	4.738696
278.199487	7729.320777	14.445965	-0.057051	4.736298
278.130259	7721.353548	14.450970	-0.057033	4.733930
278.228322	7713.299839	14.455975	-0.057046	4.731535
278.027120	7705.336072	14.460979	-0.057003	4.729166
277.905789	7697.284966	14.465984	-0.056976	4.726770
277.886013	7689.275753	14.470989	-0.056967	4.724385
277.853842	7681.357416	14.475994	-0.056956	4.722025
277.903224	7673.289981	14.480999	-0.056960	4.719620
277.752489	7665.428706	14.486003	-0.056927	4.717276
277.655609	7657.330325	14.491008	-0.056904	4.714859
277.680585	7649.244629	14.496013	-0.056903	4.712445
277.531353	7641.305626	14.501018	-0.056870	4.710074
277.562029	7633.335792	14.506023	-0.056871	4.707692
277.474301	7625.257237	14.511027	-0.056849	4.705276
277.493367	7617.363252	14.516032	-0.056848	4.702915
277.368704	7609.268665	14.521037	-0.056820	4.700492
277.352282	7601.349094	14.526042	-0.056812	4.698120
277.300387	7593.294706	14.531047	-0.056797	4.695707
277.271231	7585.300890	14.536051	-0.056786	4.693310
277.410850	7577.297931	14.541056	-0.056807	4.690910
277.284959	7569.277234	14.546061	-0.056779	4.688503
277.024174	7561.315842	14.551066	-0.056725	4.686113
276.957405	7553.312234	14.556071	-0.056707	4.683709
277.204657	7545.321215	14.561075	-0.056748	4.681306
277.104859	7537.338059	14.566080	-0.056725	4.678906
276.990251	7529.274921	14.571085	-0.056698	4.676480
277.019514	7521.229393	14.576090	-0.056698	4.674058
276.845125	7513.164994	14.581095	-0.056661	4.671629
276.793355	7505.187432	14.586099	-0.056646	4.669225
276.727036	7497.257400	14.591104	-0.056629	4.666835
276.754467	7489.226462	14.596109	-0.056629	4.664412
276.701006	7481.290254	14.601114	-0.056614	4.662017
276.748011	7473.228453	14.606119	-0.056617	4.659582
276.655300	7465.241423	14.611123	-0.056595	4.657169
276.592209	7457.272145	14.616128	-0.056578	4.654760
276.565580	7449.199871	14.621133	-0.056568	4.652319
276.554890	7441.214440	14.626138	-0.056561	4.649902
276.182959	7433.271818	14.631143	-0.056487	4.647498
276.239374	7425.208490	14.636147	-0.056492	4.645056
276.059820	7417.257624	14.641152	-0.056454	4.642646
276.244544	7409.189839	14.646157	-0.056483	4.640199
276.258390	7401.267607	14.651162	-0.056480	4.637796
276.275891	7393.222000	14.656167	-0.056478	4.635353
276.280693	7385.204232	14.661171	-0.056474	4.632918
276.338846	7377.220629	14.666176	-0.056480	4.630492
276.082121	7369.192080	14.671181	-0.056427	4.628051
276.116438	7361.192217	14.676186	-0.056428	4.625618
276.074014	7353.246628	14.681191	-0.056415	4.623199
275.830231	7345.158217	14.686195	-0.056365	4.620736
275.862086	7337.240718	14.691200	-0.056366	4.618324
275.857168	7329.170636	14.696205	-0.056360	4.615864
275.854456	7321.166268	14.701210	-0.056354	4.613422
275.718700	7313.172099	14.706215	-0.056324	4.610983
275.534434	7305.175010	14.711219	-0.056284	4.608541
275.656360	7297.167217	14.716224	-0.056302	4.606095
275.413843	7289.188877	14.721229	-0.056252	4.603656
275.438610	7281.207885	14.726234	-0.056251	4.601215
275.364402	7273.218845	14.731239	-0.056232	4.598771
275.261162	7265.163739	14.736243	-0.056208	4.596305
275.185261	7257.156820	14.741248	-0.056189	4.593852
275.242354	7249.109382	14.746253	-0.056194	4.591386
275.262186	7241.116142	14.751258	-0.056193	4.588935
275.062841	7233.116109	14.756263	-0.056151	4.586480
275.187840	7225.143581	14.761267	-0.056169	4.584033
275.226909	7217.140801	14.766272	-0.056171	4.581575
274.983516	7209.135526	14.771277	-0.056121	4.579115
275.040030	7201.163690	14.776282	-0.056126	4.576664
275.161957	7193.192966	14.781287	-0.056144	4.574212
274.871112	7185.129849	14.786291	-0.056084	4.571730
274.763012	7177.145876	14.791296	-0.056059	4.569271
274.827094	7169.077760	14.796301	-0.056066	4.566785
274.920772	7161.146571	14.801306	-0.056078	4.564340
274.751775	7153.180805	14.806311	-0.056042	4.561882
274.713365	7145.136127	14.811315	-0.056029	4.559399
274.659642	7137.177767	14.816320	-0.056014	4.556942
274.435615	7129.111121	14.821325	-0.055968	4.554449
274.544889	7121.147837	14.826330	-0.055983	4.551987
274.502535	7113.114686	14.831335	-0.055970	4.549503
274.496340	7105.110019	14.836339	-0.055964	4.547025
274.425418	7097.102922	14.841344	-0.055945	4.544546
274.516886	7089.121729	14.846349	-0.055957	4.542073
274.465601	7081.125329	14.851354	-0.055943	4.539594
274.293724	7073.189212	14.856359	-0.055905	4.537133
274.217200	7065.128296	14.861363	-0.055886	4.534631
274.270706	7057.132550	14.866368	-0.055891	4.532148
274.035357	7049.052218	14.871373	-0.055842	4.529638
273.873856	7041.130707	14.876378	-0.055807	4.527175
274.068498	7033.133359	14.881383	-0.055838	4.524688
274.136027	7025.143064	14.886387	-0.055845	4.522202
274.029525	7017.174201	14.891392	-0.055821	4.519720
273.823246	7009.134225	14.896397	-0.055777	4.517215
273.943419	7001.065723	14.901402	-0.055794	4.514700
273.805682	6993.031356	14.906407	-0.055764	4.512194
273.679814	6985.041445	14.911411	-0.055735	4.509701
273.869459	6977.071851	14.916416	-0.055765	4.507213
273.678084	6969.040329	14.921421	-0.055724	4.504703
273.782393	6961.103097	14.926426	-0.055739	4.502223
273.823200	6953.082855	14.931431	-0.055741	4.499714
273.698732	6945.082298	14.936435	-0.055713	4.497211
273.526522	6937.091610	14.941440	-0.055676	4.494708
273.572785	6929.046913	14.946445	-0.055679	4.492188
273.542299	6921.081033	14.951450	-0.055669	4.489691
273.271196	6913.073854	14.956455	-0.055613	4.487179
273.192739	6905.048734	14.961459	-0.055593	4.484661
273.403788	6897.094211	14.966464	-0.055628	4.482164
273.201070	6889.047413	14.971469	-0.055585	4.479635
273.198596	6881.079867	14.976474	-0.055579	4.477131
273.213421	6873.087848	14.981479	-0.055577	4.474617
273.228871	6864.999150	14.986483	-0.055575	4.472072
273.160223	6857.030865	14.991488	-0.055557	4.469563
272.916206	6849.061900	14.996493	-0.055506	4.467051
272.968897	6841.037083	15.001498	-0.055511	4.464522
272.986052	6833.052793	15.006503	-0.055509	4.462004
272.945802	6825.039990	15.011507	-0.055496	4.459475
273.003485	6817.063325	15.016512	-0.055502	4.456956
272.684032	6809.030073	15.021517	-0.055437	4.454417
272.547177	6800.990621	15.026522	-0.055407	4.451875
272.565395	6793.032020	15.031527	-0.055405	4.449358
272.632697	6785.024105	15.036531	-0.055413	4.446824
272.605896	6777.076047	15.041536	-0.055403	4.444307
272.419244	6769.049698	15.046541	-0.055363	4.441763
272.625174	6761.008512	15.051546	-0.055396	4.439215
272.420348	6753.002502	15.056551	-0.055353	4.436674
272.307506	6744.973467	15.061555	-0.055327	4.434126
272.338154	6736.996421	15.066560	-0.055327	4.431592
272.286027	6728.956243	15.071565	-0.055312	4.429037
272.260317	6720.973397	15.076570	-0.055302	4.426499
272.079222	6713.006040	15.081575	-0.055264	4.423964
272.206931	6704.985243	15.086579	-0.055282	4.421411
272.280151	6696.993298	15.091584	-0.055291	4.418866
271.830610	6688.978902	15.096589	-0.055202	4.416310
272.095690	6680.991591	15.101594	-0.055246	4.413764
271.859594	6672.960172	15.106599	-0.055197	4.411201
271.812121	6664.974794	15.111603	-0.055183	4.408652
271.927759	6656.989720	15.116608	-0.055200	4.406101
271.836603	6648.984955	15.121613	-0.055178	4.403543
271.781511	6641.005817	15.126618	-0.055162	4.400991
271.675869	6633.037959	15.131623	-0.055138	4.398441
271.757577	6624.993895	15.136627	-0.055148	4.395866
271.646116	6617.012096	15.141632	-0.055122	4.393308
271.621791	6608.940145	15.146637	-0.055112	4.390721
271.565090	6601.016536	15.151642	-0.055097	4.388179
271.398041	6592.988466	15.156647	-0.055060	4.385602
271.168723	6585.026472	15.161651	-0.055013	4.383044
271.316307	6576.978461	15.166656	-0.055035	4.380459
271.373695	6569.003650	15.171661	-0.055041	4.377895
271.416536	6560.986199	15.176666	-0.055043	4.375317
271.166084	6552.984323	15.181671	-0.054992	4.372740
271.056702	6544.932489	15.186675	-0.054966	4.370146
271.427027	6537.018465	15.191680	-0.055030	4.367598
271.072478	6528.982408	15.196685	-0.054959	4.365005
271.179413	6521.035859	15.201690	-0.054974	4.362442
270.929352	6513.004710	15.206695	-0.054922	4.359847
270.956867	6505.002344	15.211699	-0.054922	4.357263
271.131949	6496.972050	15.216704	-0.054950	4.354668
270.989380	6488.881017	15.221709	-0.054918	4.352051
270.986204	6480.911875	15.226714	-0.054912	4.349472
270.927445	6472.947568	15.231719	-0.054896	4.346893
270.770643	6464.910919	15.236723	-0.054862	4.344288
270.729280	6457.021323	15.241728	-0.054849	4.341730
270.659445	6448.965690	15.246733	-0.054831	4.339117
270.747773	6440.976226	15.251738	-0.054842	4.336525
270.736837	6432.963715	15.256743	-0.054835	4.333922
270.510658	6424.943110	15.261747	-0.054788	4.331315
270.638734	6416.967207	15.266752	-0.054807	4.328722
270.563592	6408.945564	15.271757	-0.054788	4.326112
270.424612	6400.974235	15.276762	-0.054757	4.323516
270.410066	6392.967766	15.281767	-0.054749	4.320908
270.203437	6384.998002	15.286771	-0.054705	4.318309
270.410798	6376.974473	15.291776	-0.054739	4.315693
270.172082	6368.928099	15.296781	-0.054689	4.313066
270.256194	6360.937978	15.301786	-0.054700	4.310457
270.251099	6352.918337	15.306791	-0.054694	4.307837
270.099122	6344.895399	15.311795	-0.054660	4.305213
270.122093	6336.986073	15.316800	-0.054660	4.302626
270.026314	6328.924959	15.321805	-0.054637	4.299986
269.974283	6320.962180	15.326810	-0.054622	4.297378
269.970069	6312.907929	15.331815	-0.054616	4.294738
269.821582	6304.913386	15.336819	-0.054583	4.292116
269.812152	6296.927197	15.341824	-0.054576	4.289495
269.545461	6288.909203	15.346829	-0.054522	4.286860
269.572956	6280.942445	15.351834	-0.054522	4.284243
269.658208	6272.933593	15.356839	-0.054532	4.281611
269.391298	6264.933422	15.361843	-0.054478	4.278977
269.410809	6256.964489	15.366848	-0.054476	4.276354
269.388976	6248.921861	15.371853	-0.054467	4.273705
269.352459	6240.890282	15.376858	-0.054455	4.271058
269.254747	6232.909718	15.381863	-0.054432	4.268426
269.246427	6224.868500	15.386867	-0.054425	4.265772
269.398388	6216.924647	15.391872	-0.054448	4.263151
269.420590	6208.883138	15.396877	-0.054447	4.260494
269.352366	6200.966044	15.401882	-0.054430	4.257877
269.356048	6192.938764	15.406887	-0.054425	4.255221
269.171403	6184.870509	15.411891	-0.054386	4.252549
269.096696	6176.911937	15.416896	-0.054367	4.249913
269.123401	6168.938698	15.421901	-0.054367	4.247271
269.087446	6160.933504	15.426906	-0.054355	4.244616
269.005587	6152.944925	15.431911	-0.054334	4.241964
269.020614	6144.894834	15.436915	-0.054332	4.239291
268.972914	6136.959565	15.441920	-0.054318	4.236654
268.658159	6128.931470	15.446925	-0.054254	4.233983
268.629420	6120.900649	15.451930	-0.054244	4.231311
268.700917	6112.914312	15.456935	-0.054252	4.228653
268.706597	6104.870172	15.461939	-0.054248	4.225974
268.490832	6096.980681	15.466944	-0.054203	4.223342
268.574699	6088.925761	15.471949	-0.054213	4.220657
268.447137	6080.985821	15.476954	-0.054185	4.218006
268.548481	6072.937768	15.481959	-0.054198	4.215319
268.576798	6064.945507	15.486963	-0.054199	4.212649
268.530500	6056.924090	15.491968	-0.054185	4.209967
268.359398	6048.938544	15.496973	-0.054148	4.207293
268.336143	6040.912744	15.501978	-0.054138	4.204606
268.234580	6032.977349	15.506983	-0.054114	4.201947
268.227345	6024.992981	15.511987	-0.054108	4.199270
268.164381	6016.972600	15.516992	-0.054091	4.196580
268.110946	6008.856680	15.521997	-0.054076	4.193855
268.202615	6000.848481	15.527002	-0.054088	4.191166
268.025424	5992.836040	15.532007	-0.054050	4.188472
267.935106	5984.868830	15.537011	-0.054028	4.185791
267.916376	5976.920298	15.542016	-0.054020	4.183116
268.019306	5968.905378	15.547021	-0.054034	4.180419
267.879745	5960.957918	15.552026	-0.054003	4.177739
267.885274	5952.911957	15.557031	-0.053998	4.175027
267.716427	5944.903640	15.562035	-0.053962	4.172323
267.744958	5936.895158	15.567040	-0.053962	4.169620
267.609419	5928.906421	15.572045	-0.053932	4.166920
267.588697	5920.890560	15.577050	-0.053923	4.164210
267.663187	5912.910026	15.582055	-0.053932	4.161511
267.541277	5904.889491	15.587059	-0.053904	4.158795
267.437616	5896.962108	15.592064	-0.053879	4.156109
267.382993	5888.886321	15.597069	-0.053864	4.153371
267.161442	5880.868428	15.602074	-0.053818	4.150649
267.218979	5872.896125	15.607079	-0.053823	4.147944
267.223787	5864.869223	15.612083	-0.053819	4.145218
267.164554	5856.913165	15.617088	-0.053803	4.142514
266.945621	5848.887973	15.622093	-0.053757	4.139783
267.381030	5840.934530	15.627098	-0.053833	4.137082
267.349770	5832.897834	15.632103	-0.053822	4.134345
267.019961	5824.866839	15.637107	-0.053756	4.131605
267.127804	5816.915642	15.642112	-0.053771	4.128895
266.935025	5808.873221	15.647117	-0.053730	4.126149
266.853315	5800.894459	15.652122	-0.053709	4.123424
266.831915	5792.915203	15.657127	-0.053700	4.120698
266.672517	5784.931593	15.662131	-0.053666	4.117967
266.663473	5776.925113	15.667136	-0.053659	4.115228
266.463913	5768.888954	15.672141	-0.053617	4.112475
266.722469	5760.849739	15.677146	-0.053660	4.109724
266.637266	5752.873041	15.682151	-0.053639	4.106989
266.322566	5744.866493	15.687155	-0.053575	4.104239
266.420020	5736.881984	15.692160	-0.053588	4.101500
266.394437	5728.892826	15.697165	-0.053578	4.098755
266.279791	5720.915099	15.702170	-0.053552	4.096012
266.313802	5712.935355	15.707175	-0.053553	4.093268
266.287578	5704.897035	15.712179	-0.053543	4.090501
266.169808	5696.913877	15.717184	-0.053516	4.087751
266.263124	5688.876449	15.722189	-0.053528	4.084982
266.117724	5680.943217	15.727194	-0.053496	4.082244
266.031552	5672.951585	15.732199	-0.053475	4.079485
266.097522	5664.957684	15.737203	-0.053482	4.076726
266.141678	5656.953769	15.742208	-0.053485	4.073961
265.967336	5648.935873	15.747213	-0.053448	4.071186
265.949378	5640.946218	15.752218	-0.053439	4.068421
265.673645	5632.944285	15.757223	-0.053383	4.065646
265.685827	5624.943674	15.762227	-0.053380	4.062874
265.677320	5616.925951	15.767232	-0.053373	4.060094
265.607138	5608.969280	15.772237	-0.053355	4.057333
265.672156	5600.925409	15.777242	-0.053362	4.054541
265.545330	5592.939763	15.782247	-0.053333	4.051764
265.267774	5584.927204	15.787251	-0.053277	4.048974
265.597134	5576.920520	15.792256	-0.053333	4.046193
265.380822	5568.932728	15.797261	-0.053287	4.043409
265.213058	5560.936881	15.802266	-0.053251	4.040621
265.191727	5552.982612	15.807271	-0.053242	4.037847
265.461888	5544.928615	15.812275	-0.053287	4.035041
265.470446	5536.832993	15.817280	-0.053284	4.032215
265.009616	5528.862894	15.822285	-0.053193	4.029423
265.170296	5520.898070	15.827290	-0.053218	4.026641
265.251416	5512.901936	15.832295	-0.053228	4.023845
264.988347	5504.904659	15.837299	-0.053174	4.021041
265.111003	5496.942828	15.842304	-0.053191	4.018253
264.954264	5488.910408	15.847309	-0.053157	4.015435
265.076911	5480.906282	15.852314	-0.053175	4.012628
264.916304	5472.901378	15.857319	-0.053140	4.009815
264.702220	5464.935595	15.862323	-0.053095	4.007013
264.693495	5456.920300	15.867328	-0.053088	4.004195
264.729215	5448.923778	15.872333	-0.053090	4.001382
264.641266	5440.953420	15.877338	-0.053068	3.998575
264.803889	5432.950091	15.882343	-0.053093	3.995757
264.673223	5424.878714	15.887347	-0.053064	3.992909
264.567982	5416.901352	15.892352	-0.053039	3.990093
264.664151	5408.887001	15.897357	-0.053052	3.987265
264.676885	5400.878550	15.902362	-0.053049	3.984435
264.318375	5392.956228	15.907367	-0.052977	3.981628
264.193988	5384.954865	15.912371	-0.052949	3.978795
264.555281	5376.971350	15.917376	-0.053011	3.975974
264.318601	5368.934596	15.922381	-0.052962	3.973122
264.100572	5360.883494	15.927386	-0.052917	3.970264
264.081215	5352.941630	15.932391	-0.052908	3.967445
264.088879	5344.914521	15.937395	-0.052904	3.964595
263.857117	5337.022089	15.942400	-0.052856	3.961786
263.854408	5328.986799	15.947405	-0.052850	3.958929
263.805801	5320.996320	15.952410	-0.052836	3.956084
263.838196	5312.954316	15.957415	-0.052837	3.953221
263.626087	5304.903511	15.962419	-0.052792	3.950348
263.671674	5296.969712	15.967424	-0.052796	3.947519
263.522385	5288.949517	15.972429	-0.052763	3.944654
263.674132	5280.984486	15.977434	-0.052786	3.941812
263.691386	5273.001969	15.982439	-0.052784	3.938959
263.563260	5264.968609	15.987443	-0.052755	3.936083
263.470718	5257.000474	15.992448	-0.052733	3.933230
263.680280	5248.939726	15.997453	-0.052767	3.930346
263.485517	5240.992635	16.002458	-0.052726	3.927493
263.476291	5233.008313	16.007463	-0.052719	3.924629
263.195800	5224.988517	16.012467	-0.052661	3.921745
263.209744	5217.023500	16.017472	-0.052659	3.918884
263.248360	5208.992758	16.022477	-0.052661	3.915997
263.210714	5200.999511	16.027482	-0.052649	3.913120
263.232066	5192.976255	16.032487	-0.052648	3.910232
262.996873	5184.993552	16.037491	-0.052599	3.907351
263.112293	5176.980870	16.042496	-0.052615	3.904464
263.055773	5169.013102	16.047501	-0.052600	3.901588
262.996269	5161.022012	16.052506	-0.052584	3.898701
262.970086	5152.994575	16.057511	-0.052574	3.895799
263.008392	5144.962909	16.062515	-0.052576	3.892895
263.049960	5136.942231	16.067520	-0.052578	3.889993
262.885612	5128.988196	16.072525	-0.052543	3.887109
262.598662	5120.972490	16.077530	-0.052484	3.884198
262.624110	5113.021424	16.082535	-0.052484	3.881314
262.669630	5105.024487	16.087539	-0.052487	3.878412
262.418370	5097.013948	16.092544	-0.052435	3.875497
262.272626	5088.774786	16.097549	-0.052403	3.872498
262.568337	5080.808531	16.102554	-0.052453	3.869606
262.272815	5072.921626	16.107559	-0.052393	3.866728
262.288126	5064.910190	16.112563	-0.052390	3.863809
262.404621	5056.972116	16.117568	-0.052407	3.860916
262.371774	5048.984716	16.122573	-0.052396	3.858001
262.158528	5040.989206	16.127578	-0.052351	3.855076
262.080814	5033.006165	16.132583	-0.052332	3.852157
262.074531	5024.951952	16.137587	-0.052325	3.849211
262.030643	5016.990371	16.142592	-0.052312	3.846295
262.026935	5009.001128	16.147597	-0.052306	3.843369
262.035910	5001.048776	16.152602	-0.052303	3.840453
261.906647	4993.055665	16.157607	-0.052274	3.837518
261.912243	4985.020459	16.162611	-0.052270	3.834568
262.008943	4977.049217	16.167616	-0.052282	3.831640
261.858252	4968.988374	16.172621	-0.052249	3.828673
261.560181	4961.028603	16.177626	-0.052189	3.825737
261.769527	4953.059253	16.182631	-0.052223	3.822806
261.492295	4945.059041	16.187635	-0.052166	3.819852
261.465661	4937.122867	16.192640	-0.052156	3.816924
261.386376	4929.072371	16.197645	-0.052136	3.813950
261.545714	4921.064428	16.202650	-0.052161	3.810995
261.652698	4913.081665	16.207655	-0.052175	3.808045
261.350986	4905.061879	16.212659	-0.052114	3.805071
261.326890	4897.119310	16.217664	-0.052105	3.802129
261.211727	4889.117436	16.222669	-0.052078	3.799161
261.047958	4881.087669	16.227674	-0.052042	3.796180
261.025721	4873.077914	16.232679	-0.052033	3.793206
260.976213	4865.008003	16.237683	-0.052019	3.790207
261.063831	4857.079172	16.242688	-0.052030	3.787261
260.977702	4849.082815	16.247693	-0.052009	3.784284
260.942534	4841.114932	16.252698	-0.051997	3.781316
260.909774	4833.102939	16.257703	-0.051986	3.778329
260.688851	4825.100101	16.262707	-0.051940	3.775340
260.759515	4817.097212	16.267712	-0.051948	3.772354
260.711190	4809.078502	16.272717	-0.051934	3.769358
260.745128	4801.097160	16.277722	-0.051935	3.766375
260.782116	4793.120281	16.282727	-0.051937	3.763391
260.476329	4785.112057	16.287731	-0.051875	3.760385
260.419296	4777.156112	16.292736	-0.051859	3.757403
260.466341	4769.112827	16.297741	-0.051863	3.754387
260.578071	4761.083689	16.302746	-0.051878	3.751376
260.731351	4753.107430	16.307751	-0.051902	3.748383
260.584879	4745.083638	16.312755	-0.051870	3.745363
260.612710	4737.147736	16.317760	-0.051870	3.742378
260.482256	4729.128473	16.322765	-0.051840	3.739355
260.299961	4721.159542	16.327770	-0.051801	3.736348
260.189064	4713.158757	16.332775	-0.051775	3.733328
260.118288	4705.117359	16.337779	-0.051757	3.730291
260.174052	4697.195248	16.342784	-0.051763	3.727299
260.184907	4689.132069	16.347789	-0.051759	3.724251
260.072723	4681.184670	16.352794	-0.051733	3.721241
260.011593	4673.216638	16.357799	-0.051717	3.718222
259.771800	4665.170901	16.362803	-0.051667	3.715167
259.938901	4657.085509	16.367808	-0.051693	3.712104
259.965020	4649.107762	16.372813	-0.051693	3.709076
259.843975	4641.124564	16.377818	-0.051665	3.706039
259.914437	4633.164428	16.382823	-0.051673	3.703014
259.769941	4625.159799	16.387827	-0.051641	3.699964
259.877730	4617.231615	16.392832	-0.051656	3.696947
259.630563	4609.196902	16.397837	-0.051605	3.693878
259.648040	4601.173097	16.402842	-0.051603	3.690818
259.705783	4593.231789	16.407847	-0.051609	3.687787
259.352973	4585.215149	16.412851	-0.051538	3.684714
259.257157	4577.261985	16.417856	-0.051515	3.681670
259.409092	4569.220932	16.422861	-0.051539	3.678596
259.083628	4561.243199	16.427866	-0.051473	3.675531
259.003285	4553.240632	16.432871	-0.051453	3.672461
259.212324	4545.216703	16.437875	-0.051487	3.669387
259.154396	4537.247194	16.442880	-0.051471	3.666324
258.991185	4529.275147	16.447885	-0.051435	3.663256
258.964967	4521.227709	16.452890	-0.051425	3.660159
259.062172	4513.254207	16.457895	-0.051438	3.657091
258.865380	4505.235841	16.462899	-0.051397	3.653996
258.943934	4497.224427	16.467904	-0.051406	3.650908
258.934822	4489.252361	16.472909	-0.051399	3.647831
258.905557	4481.244781	16.477914	-0.051389	3.644736
258.865906	4473.307675	16.482919	-0.051376	3.641666
258.789155	4465.304016	16.487923	-0.051357	3.638566
258.672661	4457.315572	16.492928	-0.051330	3.635469
258.446675	4449.269855	16.497933	-0.051283	3.632344
258.313151	4441.221599	16.502938	-0.051253	3.629218
258.471769	4433.239766	16.507943	-0.051277	3.626122
258.257709	4425.267153	16.512947	-0.051232	3.623018
258.243791	4417.268353	16.517952	-0.051225	3.619906
258.073790	4409.342595	16.522957	-0.051188	3.616815
258.130818	4401.283744	16.527962	-0.051194	3.613676
258.080451	4393.294589	16.532967	-0.051179	3.610559
258.021490	4385.312964	16.537971	-0.051163	3.607442
258.132068	4377.321564	16.542976	-0.051178	3.604322
258.072093	4369.337884	16.547981	-0.051162	3.601199
257.930658	4361.371703	16.552986	-0.051131	3.598077
257.961328	4353.350918	16.557991	-0.051131	3.594936
257.854697	4345.358829	16.562995	-0.051106	3.591800
257.946062	4337.370006	16.568000	-0.051118	3.588667
257.747309	4329.357999	16.573005	-0.051076	3.585515
257.857704	4321.396081	16.578010	-0.051092	3.582389
257.887126	4313.432610	16.583015	-0.051092	3.579256
257.633725	4305.442586	16.588019	-0.051040	3.576103
257.653716	4297.396438	16.593024	-0.051039	3.572932
257.675801	4289.365978	16.598029	-0.051037	3.569765
257.550533	4281.414199	16.603034	-0.051009	3.566621
257.492140	4273.442512	16.608039	-0.050993	3.563469
257.424362	4265.405222	16.613043	-0.050975	3.560288
257.393264	4257.464692	16.618048	-0.050965	3.557144
257.213122	4249.427160	16.623053	-0.050926	3.553954
257.263685	4241.336680	16.628058	-0.050930	3.550747
257.039140	4233.395639	16.633063	-0.050883	3.547588
257.053495	4225.365563	16.638067	-0.050881	3.544398
257.321930	4217.407831	16.643072	-0.050926	3.541241
257.096012	4209.432692	16.648077	-0.050879	3.538060
257.032826	4201.430766	16.653082	-0.050862	3.534870
256.961941	4193.457803	16.658087	-0.050843	3.531689
256.898066	4185.413348	16.663091	-0.050826	3.528477
256.800211	4177.443645	16.668096	-0.050803	3.525290
256.668604	4169.491545	16.673101	-0.050774	3.522106
256.601399	4161.515324	16.678106	-0.050756	3.518912
256.476836	4153.534365	16.683111	-0.050728	3.515712
256.335096	4145.460859	16.688115	-0.050696	3.512470
256.632039	4137.471898	16.693120	-0.050746	3.509273
256.678949	4129.459449	16.698125	-0.050750	3.506056
256.442119	4121.517962	16.703130	-0.050701	3.502856
256.425392	4113.528188	16.708135	-0.050693	3.499641
256.475480	4105.535983	16.713139	-0.050697	3.496423
256.347264	4097.573379	16.718144	-0.050668	3.493209
256.201645	4089.545273	16.723149	-0.050636	3.489965
256.340677	4081.552866	16.728154	-0.050656	3.486741
256.382980	4073.591515	16.733159	-0.050659	3.483524
256.060068	4065.581120	16.738163	-0.050594	3.480272
256.153487	4057.619051	16.743168	-0.050606	3.477051
256.249636	4049.565586	16.748173	-0.050619	3.473789
255.936329	4041.557925	16.753178	-0.050556	3.470529
255.812714	4033.605247	16.758183	-0.050528	3.467295
255.666169	4025.609665	16.763187	-0.050495	3.464040
255.867836	4017.626352	16.768192	-0.050528	3.460798
255.639322	4009.659240	16.773197	-0.050480	3.457545
255.635180	4001.636753	16.778202	-0.050474	3.454274
255.633732	3993.623187	16.783207	-0.050469	3.451004
255.431704	3985.611082	16.788211	-0.050426	3.447725
255.549413	3977.633008	16.793216	-0.050443	3.444467
255.563651	3969.636422	16.798221	-0.050441	3.441194
255.413607	3961.712451	16.803226	-0.050408	3.437943
255.336043	3953.679096	16.808231	-0.050388	3.434647
255.351834	3945.642909	16.813235	-0.050386	3.431349
255.381802	3937.658112	16.818240	-0.050386	3.428070
255.041379	3929.665490	16.823245	-0.050318	3.424772
255.193294	3921.682355	16.828250	-0.050341	3.421491
255.168870	3913.736345	16.833255	-0.050331	3.418216
255.044264	3905.692662	16.838259	-0.050303	3.414895
254.884481	3897.714177	16.843264	-0.050268	3.411596
254.961720	3889.704378	16.848269	-0.050277	3.408288
254.797096	3881.709418	16.853274	-0.050242	3.404976
255.109774	3873.790693	16.858279	-0.050295	3.401708
254.720743	3865.771097	16.863283	-0.050217	3.398371
254.549307	3857.821252	16.868288	-0.050180	3.395068
254.600056	3849.714968	16.873293	-0.050185	3.391703
254.473354	3841.716330	16.878298	-0.050156	3.388374
254.566222	3833.732025	16.883303	-0.050168	3.385056
254.708600	3825.749118	16.888307	-0.050190	3.381736
254.683930	3817.798486	16.893312	-0.050180	3.378421
254.414247	3809.811973	16.898317	-0.050125	3.375079
254.433836	3801.806126	16.903322	-0.050123	3.371735
254.605481	3793.829694	16.908327	-0.050150	3.368406
254.386205	3785.835283	16.913331	-0.050104	3.365053
254.215265	3777.870916	16.918336	-0.050067	3.361710
254.127585	3769.891100	16.923341	-0.050046	3.358360
254.128644	3761.879760	16.928346	-0.050041	3.354997
254.255195	3753.860531	16.933351	-0.050059	3.351632
253.989761	3745.850244	16.938355	-0.050005	3.348253
253.956196	3737.858647	16.943360	-0.049994	3.344887
254.124221	3729.883676	16.948365	-0.050020	3.341532
253.866420	3721.915654	16.953370	-0.049967	3.338161
254.050011	3713.909517	16.958375	-0.049996	3.334786
253.897528	3705.896238	16.963379	-0.049962	3.331393
253.889890	3697.914750	16.968384	-0.049956	3.328015
253.763164	3689.930379	16.973389	-0.049927	3.324628
253.749305	3681.974532	16.978394	-0.049919	3.321254
253.676419	3674.012094	16.983399	-0.049901	3.317871
253.473518	3665.995040	16.988403	-0.049858	3.314457
253.526320	3657.960958	16.993408	-0.049863	3.311041
253.381708	3649.974505	16.998413	-0.049831	3.307635
253.329053	3641.972867	17.003418	-0.049816	3.304222
253.531547	3634.000115	17.008423	-0.049848	3.300828
253.347812	3626.030971	17.013427	-0.049809	3.297417
253.210911	3618.064547	17.018432	-0.049778	3.294006
253.373246	3610.030971	17.023437	-0.049804	3.290574
253.290746	3602.045746	17.028442	-0.049783	3.287149
253.148089	3594.099725	17.033447	-0.049751	3.283736
252.998073	3586.077670	17.038451	-0.049718	3.280285
253.090018	3578.125170	17.043456	-0.049730	3.276871
253.176251	3570.098033	17.048461	-0.049741	3.273420
253.102441	3562.085058	17.053466	-0.049723	3.269966
253.100849	3554.127616	17.058471	-0.049717	3.266535
252.793242	3546.145524	17.063475	-0.049655	3.263078
252.790355	3538.168946	17.068480	-0.049649	3.259631
252.681979	3530.188761	17.073485	-0.049624	3.256175
252.625520	3522.151121	17.078490	-0.049608	3.252693
252.643565	3514.167145	17.083495	-0.049607	3.249232
252.388962	3506.183545	17.088499	-0.049554	3.245758
252.341738	3498.209712	17.093504	-0.049540	3.242292
252.529060	3490.207806	17.098509	-0.049570	3.238820
252.515866	3482.234296	17.103514	-0.049562	3.235348
252.495400	3474.182675	17.108519	-0.049554	3.231838
252.181261	3466.210606	17.113523	-0.049490	3.228348
252.446514	3458.166462	17.118528	-0.049534	3.224845
252.367376	3450.223582	17.123533	-0.049514	3.221369
252.018608	3442.257385	17.128538	-0.049444	3.217868
252.207940	3434.272626	17.133543	-0.049475	3.214377
252.083951	3426.277369	17.138547	-0.049446	3.210865
251.937097	3418.310119	17.143552	-0.049414	3.207360
251.864452	3410.331202	17.148557	-0.049395	3.203849
251.962410	3402.322336	17.153562	-0.049408	3.200329
251.785521	3394.388510	17.158567	-0.049371	3.196826
251.647191	3386.358667	17.163571	-0.049340	3.193278
251.580778	3378.350799	17.168576	-0.049322	3.189740
251.489074	3370.375427	17.173581	-0.049300	3.186210
251.568728	3362.371504	17.178586	-0.049310	3.182671
251.696288	3354.400760	17.183591	-0.049328	3.179145
251.305201	3346.414423	17.188595	-0.049251	3.175587
251.264106	3338.418527	17.193600	-0.049238	3.172034
251.358439	3330.412318	17.198605	-0.049250	3.168479
251.276312	3322.417970	17.203610	-0.049230	3.164918
251.140011	3314.512110	17.208615	-0.049199	3.161390
251.139464	3306.488035	17.213619	-0.049194	3.157811
251.205867	3298.482664	17.218624	-0.049201	3.154239
251.107711	3290.464568	17.223629	-0.049178	3.150650
250.841212	3282.496387	17.228634	-0.049123	3.147072
251.027131	3274.521293	17.233639	-0.049153	3.143507
251.047746	3266.506565	17.238643	-0.049152	3.139913
250.815767	3258.593738	17.243648	-0.049103	3.136349
250.613933	3250.571183	17.248653	-0.049061	3.132733
250.655857	3242.561150	17.253658	-0.049063	3.129129
250.751277	3234.581387	17.258663	-0.049076	3.125537
250.631241	3226.624332	17.263667	-0.049049	3.121942
250.713960	3218.628206	17.268672	-0.049059	3.118334
250.516497	3210.651709	17.273677	-0.049017	3.114718
250.398016	3202.647129	17.278682	-0.048990	3.111089
250.654998	3194.638139	17.283687	-0.049033	3.107470
250.572196	3186.656971	17.288691	-0.049012	3.103844
250.493192	3178.660759	17.293696	-0.048992	3.100208
250.296561	3170.730972	17.298701	-0.048951	3.096592
250.312119	3162.701653	17.303706	-0.048949	3.092936
250.138346	3154.723356	17.308711	-0.048911	3.089291
250.117720	3146.724854	17.313715	-0.048902	3.085639
250.147501	3138.763538	17.318720	-0.048903	3.082001
250.080879	3130.770172	17.323725	-0.048885	3.078341
249.891949	3122.795963	17.328730	-0.048845	3.074679
249.938933	3114.732679	17.333735	-0.048848	3.070983
249.876256	3106.727554	17.338739	-0.048832	3.067304
249.753158	3098.791811	17.343744	-0.048804	3.063650
249.840465	3090.802187	17.348749	-0.048815	3.059976
249.962230	3082.832822	17.353754	-0.048833	3.056309
249.864336	3074.852101	17.358759	-0.048809	3.052622
249.581446	3066.843933	17.363763	-0.048751	3.048909
249.633064	3058.893696	17.368768	-0.048756	3.045234
249.483713	3050.944013	17.373773	-0.048723	3.041545
249.442680	3042.959941	17.378778	-0.048710	3.037841
249.488011	3034.957243	17.383783	-0.048714	3.034128
249.376665	3026.920078	17.388787	-0.048688	3.030387
249.414728	3018.980022	17.393792	-0.048690	3.026694
249.176774	3011.007926	17.398797	-0.048640	3.022968
249.214244	3002.997802	17.403802	-0.048642	3.019233
249.153215	2995.045889	17.408807	-0.048626	3.015515
248.957491	2987.029120	17.413811	-0.048584	3.011756
249.059570	2979.048013	17.418816	-0.048598	3.008024
249.007660	2971.088205	17.423821	-0.048584	3.004289
248.914519	2963.104094	17.428826	-0.048561	3.000537
248.873440	2955.155755	17.433831	-0.048548	2.996799
248.803976	2947.106311	17.438835	-0.048530	2.993007
248.681876	2939.140187	17.443840	-0.048503	2.989247
248.478996	2931.147049	17.448845	-0.048460	2.985466
248.545072	2923.160140	17.453850	-0.048467	2.981696
248.623952	2915.190517	17.458855	-0.048477	2.977930
248.456741	2907.201059	17.463859	-0.048440	2.974138
248.429887	2899.193139	17.468864	-0.048430	2.970339
248.547638	2891.225414	17.473869	-0.048447	2.966562
248.447531	2883.248370	17.478874	-0.048423	2.962764
248.349985	2875.310171	17.483879	-0.048400	2.958980
248.199383	2867.336150	17.488883	-0.048367	2.955172
248.264441	2859.295745	17.493888	-0.048374	2.951338
248.294775	2851.296255	17.498893	-0.048375	2.947516
248.062913	2843.342532	17.503898	-0.048326	2.943699
248.095514	2835.368765	17.508903	-0.048327	2.939880
247.881289	2827.406008	17.513907	-0.048282	2.936048
247.995639	2819.399347	17.518912	-0.048298	2.932208
247.968236	2811.421087	17.523917	-0.048288	2.928369
247.896255	2803.424465	17.528922	-0.048270	2.924513
247.730788	2795.498415	17.533927	-0.048234	2.920682
247.791037	2787.492341	17.538931	-0.048240	2.916819
247.820198	2779.460883	17.543936	-0.048240	2.912937
247.696464	2771.445252	17.548941	-0.048212	2.909049
247.684087	2763.455220	17.553946	-0.048205	2.905174
247.477245	2755.553762	17.558951	-0.048161	2.901327
247.392548	2747.567312	17.563955	-0.048140	2.897440
247.559886	2739.579228	17.568960	-0.048166	2.893560
247.432581	2731.580539	17.573965	-0.048138	2.889654
247.149625	2723.613785	17.578970	-0.048080	2.885750
247.259012	2715.670660	17.583975	-0.048095	2.881873
247.225503	2707.692833	17.588979	-0.048084	2.877967
247.115525	2699.706351	17.593984	-0.048058	2.874047
246.980585	2691.688473	17.598989	-0.048028	2.870104
247.090952	2683.689861	17.603994	-0.048044	2.866179
247.026039	2675.754703	17.608999	-0.048026	2.862270
246.870262	2667.754497	17.614003	-0.047992	2.858319
246.853938	2659.792152	17.619008	-0.047984	2.854389
246.975978	2651.774099	17.624013	-0.048002	2.850433
246.885186	2643.807456	17.629018	-0.047980	2.846486
246.747689	2635.876696	17.634023	-0.047949	2.842548
246.622876	2627.899614	17.639027	-0.047921	2.838583
246.713204	2619.907523	17.644032	-0.047933	2.834616
246.483761	2611.898864	17.649037	-0.047885	2.830618
246.544985	2603.921234	17.654042	-0.047891	2.826646
246.615447	2595.938729	17.659047	-0.047899	2.822666
246.402136	2587.969180	17.664051	-0.047854	2.818671
246.406773	2579.998643	17.669056	-0.047850	2.814682
246.407189	2572.006269	17.674061	-0.047845	2.810677
246.019286	2564.061047	17.679066	-0.047768	2.806667
245.966733	2556.090172	17.684071	-0.047753	2.802658
246.031769	2548.078793	17.689075	-0.047760	2.798629
246.166380	2540.099375	17.694080	-0.047780	2.794615
246.071480	2532.094148	17.699085	-0.047757	2.790568
246.022309	2524.122456	17.704090	-0.047743	2.786536
246.122232	2516.173433	17.709095	-0.047756	2.782517
245.834322	2508.214928	17.714099	-0.047698	2.778466
245.657176	2500.249807	17.719104	-0.047660	2.774411
245.815569	2492.234719	17.724109	-0.047684	2.770345
245.706315	2484.273502	17.729114	-0.047659	2.766284
245.509971	2476.336639	17.734119	-0.047617	2.762225
245.523267	2468.332083	17.739123	-0.047614	2.758138
245.608021	2460.338340	17.744128	-0.047625	2.754054
245.388700	2452.297042	17.749133	-0.047579	2.749922
245.183298	2444.350845	17.754138	-0.047536	2.745833
245.401467	2436.383175	17.759143	-0.047571	2.741753
245.269078	2428.407304	17.764147	-0.047542	2.737641
245.060978	2420.476033	17.769152	-0.047498	2.733541
245.188650	2412.443346	17.774157	-0.047517	2.729403
245.208754	2404.469903	17.779162	-0.047515	2.725283
245.126073	2396.536361	17.784167	-0.047495	2.721171
245.092276	2388.580768	17.789171	-0.047483	2.717044
245.042711	2380.579676	17.794176	-0.047469	2.712887
244.965854	2372.598926	17.799181	-0.047450	2.708732
244.834957	2364.608764	17.804186	-0.047420	2.704562
244.924587	2356.681178	17.809191	-0.047432	2.700432
244.679134	2348.710852	17.814195	-0.047381	2.696253
244.583894	2340.720100	17.819200	-0.047358	2.692065
244.752827	2332.717834	17.824205	-0.047385	2.687882
244.640620	2324.746898	17.829210	-0.047359	2.683691
244.587371	2316.825280	17.834215	-0.047344	2.679523
244.327382	2308.860990	17.839219	-0.047290	2.675313
244.491546	2300.821423	17.844224	-0.047316	2.671084
244.536598	2292.838446	17.849229	-0.047319	2.666870
244.096326	2284.915137	17.854234	-0.047232	2.662650
244.398496	2276.922676	17.859239	-0.047283	2.658435
244.105856	2268.975719	17.864243	-0.047224	2.654198
244.124582	2260.961706	17.869248	-0.047222	2.649939
243.946036	2253.044700	17.874253	-0.047184	2.645712
243.957972	2245.039356	17.879258	-0.047181	2.641444
244.155254	2237.073883	17.884263	-0.047212	2.637202
243.817784	2229.113236	17.889267	-0.047144	2.632921
243.834830	2221.107624	17.894272	-0.047143	2.628632
243.805053	2213.156566	17.899277	-0.047132	2.624362
243.594867	2205.207336	17.904282	-0.047088	2.620074
243.658689	2197.258267	17.909287	-0.047095	2.615798
243.585569	2189.242800	17.914291	-0.047076	2.611469
243.478511	2181.290473	17.919296	-0.047051	2.607165
243.398609	2173.333848	17.924301	-0.047031	2.602854
243.507414	2165.354637	17.929306	-0.047046	2.598536
243.453935	2157.371470	17.934311	-0.047031	2.594197
243.306195	2149.223319	17.939315	-0.046998	2.589755
243.402700	2141.285175	17.944320	-0.047011	2.585437
243.539713	2133.345739	17.949325	-0.047032	2.581113
243.217220	2125.432539	17.954330	-0.046967	2.576765
243.236510	2117.474364	17.959335	-0.046965	2.572408
243.185128	2109.483369	17.964339	-0.046950	2.568022
243.061808	2101.543771	17.969344	-0.046922	2.563650
243.072868	2093.609356	17.974349	-0.046919	2.559284
242.825912	2085.664164	17.979354	-0.046868	2.554886
242.864003	2077.671365	17.984359	-0.046870	2.550474
242.782412	2069.688344	17.989363	-0.046850	2.546052
242.641672	2061.778232	17.994368	-0.046819	2.541658
242.729573	2053.798356	17.999373	-0.046830	2.537234
242.420394	2045.823934	18.004378	-0.046768	2.532777
242.400499	2037.856290	18.009383	-0.046759	2.528336
242.519369	2029.853099	18.014387	-0.046776	2.523878
242.321581	2021.939559	18.019392	-0.046734	2.519439
242.274104	2013.985491	18.024397	-0.046720	2.514981
242.207538	2005.961276	18.029402	-0.046702	2.510473
242.438111	1997.967764	18.034407	-0.046740	2.505997
241.982104	1990.056667	18.039411	-0.046650	2.501509
242.239058	1982.070781	18.044416	-0.046693	2.497022
242.272929	1974.108517	18.049421	-0.046694	2.492525
242.024854	1966.138591	18.054426	-0.046643	2.487994
241.895339	1958.210071	18.059431	-0.046614	2.483488
241.697963	1950.261164	18.064435	-0.046572	2.478956
241.768241	1942.294122	18.069440	-0.046580	2.474426
241.715581	1934.301253	18.074445	-0.046565	2.469864
241.597297	1926.322706	18.079450	-0.046538	2.465296
241.567675	1918.401953	18.084455	-0.046528	2.460759
241.440704	1910.442707	18.089459	-0.046499	2.456185
241.462524	1902.465353	18.094464	-0.046498	2.451603
241.341701	1894.493649	18.099469	-0.046470	2.447005
241.332337	1886.533750	18.104474	-0.046463	2.442414
241.266111	1878.607075	18.109479	-0.046446	2.437828
241.304179	1870.590860	18.114483	-0.046448	2.433190
241.196713	1862.582701	18.119488	-0.046423	2.428537
241.183305	1854.640616	18.124493	-0.046415	2.423921
241.176933	1846.686485	18.129498	-0.046409	2.419289
241.231893	1838.731990	18.134503	-0.046414	2.414653
240.988249	1830.768489	18.139507	-0.046364	2.409979
241.179745	1822.786863	18.144512	-0.046394	2.405320
241.042800	1814.877730	18.149517	-0.046364	2.400668
240.802075	1806.948731	18.154522	-0.046314	2.395988
240.778445	1798.962784	18.159527	-0.046305	2.391282
240.710293	1790.995066	18.164531	-0.046287	2.386574
240.667045	1783.060084	18.169536	-0.046274	2.381878
240.608247	1775.114427	18.174541	-0.046258	2.377165
240.386196	1767.149427	18.179546	-0.046211	2.372418
240.702111	1759.151941	18.184551	-0.046265	2.367685
240.558501	1751.215993	18.189555	-0.046233	2.362943
240.432985	1743.297543	18.194560	-0.046205	2.358203
240.335378	1735.332184	18.199565	-0.046181	2.353427
240.294469	1727.327817	18.204570	-0.046169	2.348623
240.138819	1719.403606	18.209575	-0.046135	2.343848
240.177700	1711.424780	18.214579	-0.046137	2.339047
240.061640	1703.491820	18.219584	-0.046110	2.334250
239.988772	1695.539201	18.224589	-0.046092	2.329435
239.929938	1687.566414	18.229594	-0.046076	2.324599
240.003734	1679.642020	18.234599	-0.046084	2.319793
239.790459	1671.699550	18.239603	-0.046039	2.314943
239.827781	1663.709489	18.244608	-0.046041	2.310074
239.945363	1655.737519	18.249613	-0.046058	2.305213
239.558991	1647.841556	18.254618	-0.045981	2.300345
239.602954	1639.892658	18.259623	-0.045984	2.295471
239.435574	1631.921646	18.264627	-0.045948	2.290555
239.680263	1623.936778	18.269632	-0.045989	2.285655
239.577620	1616.017912	18.274637	-0.045964	2.280756
239.351551	1608.093321	18.279642	-0.045917	2.275832
239.552325	1600.050447	18.284647	-0.045949	2.270860
239.279687	1592.107512	18.289651	-0.045894	2.265899
239.149620	1584.186946	18.294656	-0.045864	2.260953
239.338526	1576.219104	18.299661	-0.045895	2.255995
239.210659	1568.268988	18.304666	-0.045866	2.251009
239.115922	1560.336929	18.309671	-0.045843	2.246026
239.059856	1552.403994	18.314675	-0.045827	2.241035
239.104178	1544.457440	18.319680	-0.045831	2.236033
238.943009	1536.515807	18.324685	-0.045796	2.231005
238.888301	1528.546743	18.329690	-0.045780	2.225958
238.934315	1520.610694	18.334695	-0.045784	2.220929
238.872366	1512.674587	18.339699	-0.045767	2.215878
238.546754	1504.761539	18.344704	-0.045702	2.210808
238.515104	1496.806509	18.349709	-0.045691	2.205725
238.462390	1488.851592	18.354714	-0.045676	2.200629
238.457108	1480.930558	18.359719	-0.045670	2.195547
238.309241	1472.953406	18.364723	-0.045637	2.190404
238.532309	1464.963231	18.369728	-0.045674	2.185274
238.479499	1457.050944	18.374733	-0.045659	2.180157
238.093726	1449.140866	18.379738	-0.045582	2.174999
238.054577	1441.195113	18.384743	-0.045569	2.169838
238.002369	1433.245211	18.389747	-0.045555	2.164660
237.951248	1425.321845	18.394752	-0.045540	2.159487
237.886769	1417.389817	18.399757	-0.045523	2.154295
237.776567	1409.415188	18.404762	-0.045497	2.149059
237.821760	1401.489121	18.409767	-0.045501	2.143855
237.781925	1393.552031	18.414771	-0.045488	2.138624
237.876831	1385.584610	18.419776	-0.045501	2.133373
237.677587	1377.667832	18.424781	-0.045459	2.128115
237.483773	1369.749056	18.429786	-0.045418	2.122842
237.484424	1361.831958	18.434791	-0.045413	2.117576
237.366871	1353.854056	18.439795	-0.045386	2.112245
237.138503	1345.890186	18.444800	-0.045338	2.106900
237.115952	1337.970232	18.449805	-0.045329	2.101589
237.118569	1330.022565	18.454810	-0.045324	2.096250
236.971359	1322.112420	18.459815	-0.045292	2.090907
236.838415	1314.167882	18.464819	-0.045262	2.085529
236.762313	1306.248560	18.469824	-0.045243	2.080159
236.941874	1298.308425	18.474829	-0.045271	2.074787
236.726356	1290.363054	18.479834	-0.045226	2.069358
236.717072	1282.440145	18.484839	-0.045219	2.063950
236.731740	1274.507829	18.489843	-0.045217	2.058525
236.617940	1266.580397	18.494848	-0.045191	2.053075
236.650397	1258.640437	18.499853	-0.045192	2.047617
236.545632	1250.714128	18.504858	-0.045167	2.042140
236.585585	1242.810452	18.509863	-0.045170	2.036678
236.314569	1234.882999	18.514867	-0.045114	2.031154
236.358766	1226.927349	18.519872	-0.045117	2.025627
236.247187	1219.031499	18.524877	-0.045091	2.020111
236.099170	1211.112258	18.529882	-0.045059	2.014559
235.986841	1203.168754	18.534887	-0.045033	2.008979
236.124349	1195.222414	18.539891	-0.045053	2.003407
235.892498	1187.347867	18.544896	-0.045005	1.997832
235.818272	1179.416523	18.549901	-0.044986	1.992217
235.712135	1171.477787	18.554906	-0.044961	1.986578
235.774452	1163.554589	18.559911	-0.044968	1.980952
235.507173	1155.667241	18.564915	-0.044913	1.975300
235.514915	1147.722648	18.569920	-0.044910	1.969621
235.652400	1139.783096	18.574925	-0.044930	1.963942
235.581749	1131.885543	18.579930	-0.044912	1.958255
235.598481	1123.947102	18.584935	-0.044910	1.952531
235.305217	1116.021447	18.589939	-0.044850	1.946766
235.321589	1108.088722	18.594944	-0.044848	1.941012
235.282181	1100.194491	18.599949	-0.044836	1.935263
235.079147	1092.275289	18.604954	-0.044793	1.929461
235.227918	1084.344745	18.609959	-0.044816	1.923672
235.009033	1076.470634	18.614963	-0.044770	1.917866
234.874156	1068.547102	18.619968	-0.044740	1.912015
235.079018	1060.594021	18.624973	-0.044773	1.906162
234.901701	1052.707644	18.629978	-0.044735	1.900298
234.833830	1044.824109	18.634983	-0.044717	1.894430
234.651034	1036.908887	18.639987	-0.044678	1.888508
234.721929	1028.982368	18.644992	-0.044686	1.882587
234.728667	1021.100002	18.649997	-0.044683	1.876673
234.449760	1013.196503	18.655002	-0.044626	1.870691
234.431821	1005.276213	18.660007	-0.044617	1.864708
234.309549	997.389230	18.665011	-0.044589	1.858719
234.201745	989.485335	18.670016	-0.044564	1.852699
234.290477	981.559932	18.675021	-0.044576	1.846666
234.153073	973.669710	18.680026	-0.044545	1.840614
234.345167	965.756785	18.685031	-0.044576	1.834563
234.247323	957.843881	18.690035	-0.044553	1.828458
233.944212	949.984393	18.695040	-0.044491	1.822349
233.987275	942.083291	18.700045	-0.044494	1.816229
233.908589	934.168422	18.705050	-0.044474	1.810062
234.027320	926.272627	18.710055	-0.044492	1.803913
233.928108	918.391338	18.715059	-0.044468	1.797728
233.739255	910.484873	18.720064	-0.044428	1.791492
233.708784	902.567295	18.725069	-0.044417	1.785243
233.421520	894.716090	18.730074	-0.044359	1.778994
233.532455	886.809629	18.735079	-0.044374	1.772728
233.452405	878.910443	18.740083	-0.044354	1.766422
233.303987	871.053064	18.745088	-0.044322	1.760118
233.119672	863.197499	18.750093	-0.044282	1.753789
233.041926	855.283577	18.755098	-0.044263	1.747402
233.013706	847.411483	18.760103	-0.044253	1.741033
232.973022	839.530194	18.765107	-0.044240	1.734631
232.844116	831.637116	18.770112	-0.044211	1.728184
232.987388	823.750666	18.775117	-0.044233	1.721754
232.808333	815.896862	18.780122	-0.044194	1.715285
232.746143	808.007146	18.785127	-0.044178	1.708776
232.717981	800.118399	18.790131	-0.044167	1.702248
232.571000	792.262294	18.795136	-0.044135	1.695707
232.614698	784.374149	18.800141	-0.044138	1.689138
232.497763	776.511626	18.805146	-0.044111	1.682544
232.587979	768.633845	18.810151	-0.044123	1.675939
232.491446	760.765944	18.815155	-0.044100	1.669291
232.269366	752.921373	18.820160	-0.044054	1.662619
232.249166	745.063193	18.825165	-0.044045	1.655936
232.102431	737.196952	18.830170	-0.044013	1.649202
231.988256	729.354108	18.835175	-0.043986	1.642465
231.939782	721.505146	18.840179	-0.043972	1.635704
231.894395	713.575288	18.845184	-0.043959	1.628845
231.901254	705.718386	18.850189	-0.043955	1.622027
231.592751	697.902355	18.855194	-0.043893	1.615173
231.692728	690.020157	18.860199	-0.043906	1.608288
231.549009	682.182791	18.865203	-0.043875	1.601379
231.392216	674.360785	18.870208	-0.043840	1.594452
231.428623	666.482431	18.875213	-0.043842	1.587472
231.526343	658.616327	18.880218	-0.043855	1.580481
231.225780	650.837181	18.885223	-0.043794	1.573479
231.263001	642.958509	18.890227	-0.043796	1.566406
231.190498	635.140964	18.895232	-0.043778	1.559339
231.183435	627.301896	18.900237	-0.043772	1.552230
231.001151	619.457273	18.905242	-0.043733	1.545058
230.892158	611.661143	18.910247	-0.043707	1.537908
230.829786	603.800920	18.915251	-0.043691	1.530672
230.727279	595.985212	18.920256	-0.043667	1.523436
230.831354	588.152591	18.925261	-0.043681	1.516182
230.696496	580.320853	18.930266	-0.043651	1.508857
230.455407	572.540708	18.935271	-0.043601	1.501529
230.558739	564.695721	18.940275	-0.043615	1.494157
230.458361	556.878107	18.945280	-0.043592	1.486742
230.299851	549.104931	18.950285	-0.043557	1.479324
230.129171	541.275924	18.955290	-0.043520	1.471812
230.221641	533.420338	18.960295	-0.043533	1.464278
230.216778	525.619009	18.965299	-0.043527	1.456742
229.865622	517.855860	18.970304	-0.043457	1.449149
229.909519	510.053242	18.975309	-0.043460	1.441540
229.907751	502.250782	18.980314	-0.043454	1.433884
229.730701	494.467821	18.985319	-0.043416	1.426178
229.632907	486.690406	18.990323	-0.043393	1.418448
229.446382	478.919644	18.995328	-0.043354	1.410668
229.535028	471.123818	19.000333	-0.043365	1.402865
229.335932	463.367097	19.005338	-0.043323	1.395009
229.335702	455.559356	19.010343	-0.043318	1.387091
229.135018	447.814404	19.015347	-0.043276	1.379158
228.980629	440.046677	19.020352	-0.043242	1.371163
229.105459	432.257032	19.025357	-0.043260	1.363146
229.143168	424.485588	19.030362	-0.043263	1.355086
228.973694	416.738715	19.035367	-0.043226	1.346967
228.654146	409.039263	19.040371	-0.043162	1.338823
228.620001	401.273201	19.045376	-0.043150	1.330608
228.656545	393.520480	19.050381	-0.043152	1.322370
228.380290	385.787521	19.055386	-0.043096	1.314044
228.500753	377.913002	19.060391	-0.043113	1.305584
228.414426	370.205364	19.065395	-0.043092	1.297213
228.308690	362.489170	19.070400	-0.043068	1.288775
228.176725	354.796465	19.075405	-0.043038	1.280302
227.971115	347.104430	19.080410	-0.042995	1.271759
228.092706	339.364276	19.085415	-0.043013	1.263166
227.875104	331.700122	19.090419	-0.042967	1.254536
227.927234	323.970390	19.095424	-0.042972	1.245823
227.780601	316.314416	19.100429	-0.042940	1.237095
227.401920	308.645831	19.105434	-0.042865	1.228244
227.318764	300.968001	19.110439	-0.042844	1.219377
227.271022	293.276648	19.115443	-0.042830	1.210436
227.250567	285.596202	19.120448	-0.042822	1.201447
227.056550	277.960114	19.125453	-0.042781	1.192407
226.844402	270.309376	19.130458	-0.042736	1.183277
226.975006	262.636602	19.135463	-0.042756	1.174120
226.746866	255.004068	19.140467	-0.042708	1.164865
226.691274	247.377519	19.145472	-0.042693	1.155579
226.489535	239.732058	19.150477	-0.042651	1.146164
225.986377	232.163614	19.155482	-0.042552	1.136703
225.780459	224.559379	19.160487	-0.042509	1.127181
225.885573	216.923858	19.165491	-0.042524	1.117605
225.418842	209.374307	19.170496	-0.042432	1.107931
225.299303	201.791726	19.175501	-0.042405	1.098206
224.816638	194.259130	19.180506	-0.042310	1.088378
224.637351	186.703368	19.185511	-0.042272	1.078498
224.078659	179.192755	19.190515	-0.042163	1.068500
223.756534	171.661032	19.195520	-0.042099	1.058433
223.518594	164.118846	19.200525	-0.042050	1.048275
223.157702	156.615136	19.205530	-0.041978	1.038041
222.693130	149.141466	19.210535	-0.041886	1.027721
222.204741	141.675947	19.215539	-0.041791	1.017302
221.861915	134.190250	19.220544	-0.041722	1.006782
221.609620	126.726098	19.225549	-0.041670	0.996204
221.072568	119.256888	19.230554	-0.041566	0.985433
220.507972	111.853649	19.235559	-0.041456	0.974632
220.113278	104.419166	19.240563	-0.041377	0.963707
219.648365	97.027718	19.245568	-0.041286	0.952703
219.387457	89.610559	19.250573	-0.041233	0.941584
218.918776	82.240492	19.255578	-0.041141	0.930348
218.345525	74.914889	19.260583	-0.041030	0.919015
217.941453	67.555015	19.265587	-0.040950	0.907533
217.365517	60.483936	19.270592	-0.040838	0.896311