Tue Mar 23 11:20:36 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.657747	0.126263	0.000000	0.000034	0.723339

0.554772	0.148269	0.005005	0.000053	0.723347
0.291037	0.193797	0.010010	0.000102	0.723344
0.613850	0.140088	0.015014	0.000042	0.723352
0.664476	0.111472	0.020019	0.000032	0.723313
0.699193	-0.049927	0.025024	0.000026	0.723009
0.618217	-0.033111	0.030029	0.000041	0.723014
0.513592	-0.018888	0.035034	0.000060	0.723006
0.551806	-0.019194	0.040038	0.000053	0.723019
0.450803	-0.005058	0.045043	0.000072	0.723011
0.865435	-0.079412	0.050048	-0.000006	0.723010
0.688458	-0.048570	0.055053	0.000027	0.723009
0.472672	-0.012212	0.060058	0.000067	0.723005
0.610702	-0.033349	0.065062	0.000041	0.723012
0.690700	-0.051593	0.070067	0.000026	0.723005
0.849726	-0.078735	0.075072	-0.000003	0.723007
0.738434	-0.057160	0.080077	0.000017	0.723011
0.656705	-0.102214	0.085082	0.000032	0.722894
0.660586	-0.199833	0.090086	0.000032	0.722704
0.470940	-0.172102	0.095091	0.000067	0.722692
0.663775	-0.201964	0.100096	0.000031	0.722701
0.735831	-0.215612	0.105101	0.000017	0.722700
0.343645	-0.148327	0.110106	0.000090	0.722695
0.410102	-0.155810	0.115110	0.000078	0.722704
0.451113	-0.286364	0.120115	0.000070	0.722462
0.556101	-0.350465	0.125120	0.000050	0.722373
0.597533	-0.356159	0.130125	0.000043	0.722377
0.568668	-0.353351	0.135130	0.000048	0.722372
0.714523	-0.374932	0.140134	0.000021	0.722381
0.565299	-0.467195	0.145139	0.000048	0.722148
0.693119	-0.524140	0.150144	0.000024	0.722081
0.668507	-0.520222	0.155149	0.000029	0.722080
0.438616	-0.481665	0.160154	0.000072	0.722076
0.391889	-0.562658	0.165158	0.000080	0.721901
0.298052	-0.625356	0.170163	0.000098	0.721745
0.501304	-0.659066	0.175168	0.000060	0.721750
0.215338	-0.608301	0.180173	0.000113	0.721750
0.242730	-0.715628	0.185178	0.000108	0.721549
0.543214	-0.820590	0.190182	0.000052	0.721448
0.338903	-0.788965	0.195187	0.000090	0.721438
0.292552	-0.802447	0.200192	0.000098	0.721396
0.563091	-0.987409	0.205197	0.000048	0.721127
0.497228	-0.980033	0.210202	0.000060	0.721119
0.511297	-0.985302	0.215206	0.000057	0.721113
0.426142	-1.089950	0.220211	0.000073	0.720878
0.410558	-1.086766	0.225216	0.000076	0.720879
0.335547	-1.093107	0.230221	0.000090	0.720840
0.347253	-1.248213	0.235226	0.000087	0.720539
0.378658	-1.249272	0.240230	0.000081	0.720548
0.013371	-1.244744	0.245235	0.000149	0.720429
0.156290	-1.373364	0.250240	0.000123	0.720226
0.439174	-1.423480	0.255245	0.000070	0.720227
0.120578	-1.482178	0.260250	0.000129	0.720000
-0.095850	-1.490839	0.265254	0.000169	0.719907
0.063219	-1.532970	0.270259	0.000140	0.719880
0.099257	-1.679022	0.275264	0.000133	0.719605
0.059534	-1.671857	0.280269	0.000140	0.719605
0.151410	-1.795111	0.285274	0.000123	0.719395
0.190319	-1.861186	0.290278	0.000116	0.719278
0.174627	-1.913018	0.295283	0.000119	0.719171
0.219539	-2.025196	0.300288	0.000110	0.718966
0.008079	-2.002717	0.305293	0.000150	0.718936
0.131037	-2.173354	0.310298	0.000127	0.718642
-0.444861	-2.066087	0.315302	0.000234	0.718652
-0.617886	-2.165819	0.320307	0.000266	0.718394
-0.648047	-2.179207	0.325312	0.000271	0.718358
-1.271826	-2.158993	0.330317	0.000387	0.718178
-2.483620	-2.024523	0.335322	0.000613	0.718018
-2.616518	-1.998277	0.340326	0.000637	0.718023
-2.858169	-2.062844	0.345331	0.000682	0.717811
-3.779910	-1.952185	0.350336	0.000854	0.717705
-3.379232	-2.021078	0.355341	0.000779	0.717710
-3.855964	-1.987210	0.360346	0.000868	0.717609
-4.275852	-2.025731	0.365350	0.000946	0.717386
-4.053802	-2.071576	0.370355	0.000904	0.717373
-4.693723	-1.955788	0.375360	0.001023	0.717377
-4.655026	-2.057554	0.380365	0.001016	0.717190
-5.396130	-1.982361	0.385370	0.001154	0.717078
-5.132150	-2.024470	0.390374	0.001105	0.717087
-5.322191	-1.993295	0.395379	0.001140	0.717082
-5.428844	-2.073276	0.400384	0.001160	0.716887
-6.518128	-1.943577	0.405389	0.001362	0.716760
-6.392467	-1.970911	0.410394	0.001339	0.716750
-6.024089	-2.033074	0.415398	0.001270	0.716757
-6.314291	-1.984651	0.420403	0.001324	0.716751
-6.855187	-2.032922	0.425408	0.001425	0.716465
-7.090257	-1.996955	0.430413	0.001468	0.716453
-7.294892	-1.965542	0.435418	0.001506	0.716443
-7.179739	-1.981230	0.440422	0.001485	0.716453
-7.708172	-1.892819	0.445427	0.001583	0.716442
-7.565611	-2.026505	0.450432	0.001557	0.716228
-7.939401	-2.006559	0.455437	0.001626	0.716136
-8.445788	-1.919077	0.460442	0.001720	0.716131
-7.952506	-2.002783	0.465446	0.001628	0.716139
-8.141295	-1.972770	0.470451	0.001663	0.716132
-8.029335	-2.012746	0.475456	0.001642	0.716092
-8.559229	-2.022517	0.480461	0.001741	0.715886
-8.779791	-1.986608	0.485466	0.001782	0.715880
-8.690165	-1.999408	0.490470	0.001765	0.715886
-8.837800	-1.976920	0.495475	0.001792	0.715879
-8.481117	-2.038820	0.500480	0.001726	0.715882
-8.917861	-2.083491	0.505485	0.001807	0.715640
-10.099023	-1.922694	0.510490	0.002027	0.715542
-9.584294	-2.009361	0.515494	0.001931	0.715552
-9.510876	-2.026518	0.520499	0.001917	0.715544
-10.070478	-1.926088	0.525504	0.002021	0.715546
-9.624286	-2.003540	0.530509	0.001938	0.715550
-9.819910	-2.086570	0.535514	0.001974	0.715316
-10.850681	-1.943327	0.540518	0.002166	0.715236
-11.031155	-1.916559	0.545523	0.002200	0.715226
-10.714563	-1.969710	0.550528	0.002141	0.715233
-10.646513	-1.981976	0.555533	0.002128	0.715233
-10.831809	-1.953523	0.560538	0.002162	0.715224
-10.987613	-1.921315	0.565542	0.002191	0.715233
-11.351943	-2.021030	0.570547	0.002259	0.714906
-11.620673	-1.971462	0.575552	0.002309	0.714910
-11.662281	-1.962781	0.580557	0.002316	0.714913
-11.757068	-1.950446	0.585562	0.002334	0.714904
-11.644887	-1.966405	0.590566	0.002313	0.714912
-11.971438	-1.912003	0.595571	0.002374	0.714905
-11.933477	-1.917730	0.600576	0.002366	0.714907
-12.236193	-2.007353	0.605581	0.002423	0.714622
-12.820705	-1.912817	0.610586	0.002531	0.714603
-12.530599	-1.959645	0.615590	0.002477	0.714613
-12.554985	-1.958512	0.620595	0.002482	0.714607
-12.820273	-1.909910	0.625600	0.002531	0.714610
-12.569349	-1.953139	0.630605	0.002484	0.714613
-12.460044	-1.976526	0.635610	0.002464	0.714605
-12.946418	-2.038675	0.640614	0.002554	0.714310
-13.895467	-1.887056	0.645619	0.002731	0.714276
-13.608204	-1.938251	0.650624	0.002677	0.714276
-13.036685	-2.037448	0.655629	0.002571	0.714281
-13.750326	-1.915504	0.660634	0.002703	0.714271
-13.694353	-1.920552	0.665638	0.002693	0.714281
-13.664702	-1.930417	0.670643	0.002687	0.714272
-13.972932	-1.990613	0.675648	0.002745	0.714044
-14.640392	-1.910815	0.680653	0.002869	0.713966
-14.687705	-1.904770	0.685658	0.002877	0.713962
-14.212473	-1.984071	0.690662	0.002789	0.713973
-14.459236	-1.943833	0.695667	0.002835	0.713965
-14.534213	-1.928699	0.700672	0.002849	0.713969
-14.280587	-1.972962	0.705677	0.002801	0.713971
-14.641165	-1.990024	0.710682	0.002868	0.713810
-15.277189	-1.953409	0.715686	0.002987	0.713657
-15.154835	-1.979510	0.720691	0.002964	0.713649
-15.623489	-1.894798	0.725696	0.003051	0.713652
-15.559899	-1.903563	0.730701	0.003039	0.713657
-15.256802	-1.963429	0.735706	0.002982	0.713646
-15.188977	-1.970397	0.740710	0.002970	0.713656
-15.472598	-1.970171	0.745715	0.003022	0.713556
-16.351022	-1.912549	0.750720	0.003186	0.713360
-15.801610	-2.008994	0.755725	0.003083	0.713363
-16.418661	-1.903065	0.760730	0.003198	0.713355
-16.347963	-1.911449	0.765734	0.003185	0.713364
-16.247529	-1.933094	0.770739	0.003166	0.713356
-16.207138	-1.937728	0.775744	0.003158	0.713362
-16.159350	-1.994985	0.780749	0.003149	0.713265
-17.587109	-1.864396	0.785754	0.003415	0.713019
-17.135270	-1.942209	0.790758	0.003331	0.713024
-17.450073	-1.887216	0.795763	0.003389	0.713022
-17.339047	-1.908197	0.800768	0.003369	0.713020
-16.834926	-1.995363	0.805773	0.003275	0.713026
-17.371087	-1.903172	0.810778	0.003374	0.713019
-17.108376	-1.944745	0.815782	0.003325	0.713030
-17.185568	-2.045452	0.820787	0.003340	0.712802
-18.393415	-1.876753	0.825792	0.003564	0.712710
-18.312192	-1.889486	0.830797	0.003549	0.712714
-18.140929	-1.924686	0.835802	0.003517	0.712704
-17.918494	-1.960185	0.840806	0.003476	0.712713
-18.229057	-1.907513	0.845811	0.003533	0.712708
-18.174274	-1.917692	0.850816	0.003523	0.712707
-17.946089	-2.032273	0.855821	0.003480	0.712560
-19.189248	-1.900118	0.860826	0.003712	0.712382
-18.932671	-1.942407	0.865830	0.003664	0.712389
-19.227532	-1.892570	0.870835	0.003719	0.712384
-19.154714	-1.907841	0.875840	0.003705	0.712380
-18.911760	-1.947469	0.880845	0.003660	0.712387
-19.148169	-1.908866	0.885850	0.003704	0.712381
-18.990538	-1.964825	0.890854	0.003674	0.712325
-19.764814	-1.945220	0.895859	0.003818	0.712090
-19.748270	-1.949213	0.900864	0.003815	0.712088
-19.648613	-1.964959	0.905869	0.003796	0.712092
-19.967083	-1.912909	0.910874	0.003855	0.712083
-20.212875	-1.865664	0.915878	0.003901	0.712090
-20.121875	-1.883665	0.920883	0.003884	0.712087
-20.021608	-1.901398	0.925888	0.003865	0.712087
-20.337580	-1.995062	0.930893	0.003924	0.711788
-21.243450	-1.852018	0.935898	0.004093	0.711752
-20.855055	-1.916545	0.940902	0.004020	0.711761
-20.416501	-1.998265	0.945907	0.003938	0.711754
-21.016166	-1.889384	0.950912	0.004050	0.711759
-20.943222	-1.900372	0.955917	0.004036	0.711763
-20.807258	-1.928144	0.960922	0.004011	0.711756
-20.901159	-2.011809	0.965926	0.004028	0.711556
-21.641781	-1.932036	0.970931	0.004166	0.711452
-21.498755	-1.958367	0.975936	0.004139	0.711451
-21.393779	-1.974241	0.980941	0.004120	0.711457
-22.181870	-1.838204	0.985946	0.004266	0.711448
-21.559902	-1.944074	0.990950	0.004150	0.711458
-21.624477	-1.937017	0.995955	0.004162	0.711449
-22.365051	-1.926227	1.000960	0.004300	0.711208
-22.670861	-1.904928	1.005965	0.004357	0.711142
-22.521138	-1.935815	1.010970	0.004329	0.711134
-22.449073	-1.945358	1.015974	0.004315	0.711140
-22.811056	-1.883709	1.020979	0.004383	0.711135
-22.429584	-1.951662	1.025984	0.004311	0.711135
-22.376776	-1.957227	1.030989	0.004302	0.711143
-23.099043	-1.899960	1.035994	0.004436	0.711001
-23.400499	-1.908936	1.040998	0.004492	0.710876
-23.107708	-1.964100	1.046003	0.004437	0.710870
-23.477890	-1.897000	1.051008	0.004506	0.710873
-23.449880	-1.900142	1.056013	0.004501	0.710876
-23.222185	-1.944060	1.061018	0.004458	0.710870
-23.249407	-1.933649	1.066022	0.004463	0.710881
-23.761101	-1.973612	1.071027	0.004558	0.710620
-24.431504	-1.896815	1.076032	0.004683	0.710535
-24.144372	-1.944564	1.081037	0.004630	0.710542
-24.326463	-1.916797	1.086042	0.004663	0.710532
-24.244676	-1.927959	1.091046	0.004648	0.710539
-24.326175	-1.915380	1.096051	0.004663	0.710536
-24.494067	-1.886548	1.101056	0.004694	0.710534
-24.647812	-1.962571	1.106061	0.004723	0.710327
-25.503929	-1.867033	1.111066	0.004882	0.710214
-25.373540	-1.885802	1.116070	0.004858	0.710223
-25.535689	-1.858774	1.121075	0.004888	0.710219
-25.296113	-1.901801	1.126080	0.004843	0.710219
-25.127828	-1.929157	1.131085	0.004812	0.710224
-25.453702	-1.875378	1.136090	0.004872	0.710216
-25.152172	-1.961616	1.141094	0.004816	0.710151
-25.677583	-1.996492	1.146099	0.004914	0.709894
-26.355817	-1.877429	1.151104	0.005040	0.709891
-26.510583	-1.846875	1.156109	0.005068	0.709897
-25.938532	-1.951094	1.161114	0.004962	0.709893
-25.945935	-1.947149	1.166118	0.004963	0.709898
-26.583289	-1.834979	1.171123	0.005082	0.709896
-26.363668	-1.875388	1.176128	0.005041	0.709893
-26.533846	-1.984198	1.181133	0.005072	0.709615
-27.334107	-1.852438	1.186138	0.005221	0.709594
-27.092432	-1.892681	1.191142	0.005176	0.709600
-26.760807	-1.954647	1.196147	0.005114	0.709594
-27.084242	-1.895873	1.201152	0.005174	0.709597
-26.879299	-1.930546	1.206157	0.005136	0.709601
-26.800059	-1.958853	1.211162	0.005121	0.709572
-27.620999	-1.965015	1.216166	0.005274	0.709268
-27.932971	-1.912378	1.221171	0.005332	0.709262
-27.979688	-1.904549	1.226176	0.005340	0.709261
-27.471881	-1.993229	1.231181	0.005246	0.709265
-28.042377	-1.893785	1.236186	0.005352	0.709261
-28.133067	-1.873208	1.241190	0.005369	0.709270
-27.819925	-1.937885	1.246195	0.005310	0.709252
-28.689365	-1.932679	1.251200	0.005472	0.708953
-28.832286	-1.902328	1.256205	0.005499	0.708963
-29.126010	-1.856292	1.261210	0.005553	0.708950
-28.755228	-1.918454	1.266214	0.005484	0.708958
-28.864835	-1.901055	1.271219	0.005504	0.708954
-29.055753	-1.867336	1.276224	0.005540	0.708954
-28.504148	-1.960900	1.281229	0.005437	0.708963
-29.207428	-1.966068	1.286234	0.005568	0.708702
-29.899013	-1.872467	1.291238	0.005696	0.708643
-29.654954	-1.918166	1.296243	0.005651	0.708639
-29.838092	-1.886027	1.301248	0.005685	0.708638
-30.023579	-1.849925	1.306253	0.005719	0.708644
-29.914361	-1.873622	1.311258	0.005699	0.708636
-29.673511	-1.913841	1.316262	0.005654	0.708642
-29.664600	-1.974898	1.321267	0.005652	0.708523
-30.695734	-1.879815	1.326272	0.005844	0.708345
-30.094970	-1.983005	1.331277	0.005732	0.708353
-30.875241	-1.848623	1.336282	0.005877	0.708344
-30.776964	-1.861958	1.341286	0.005859	0.708353
-30.382900	-1.934895	1.346291	0.005785	0.708348
-30.798865	-1.860798	1.351296	0.005863	0.708348
-30.729826	-1.943561	1.356301	0.005850	0.708207
-31.868574	-1.841281	1.361306	0.006062	0.708005
-31.184376	-1.959266	1.366310	0.005934	0.708013
-31.507662	-1.902889	1.371315	0.005994	0.708011
-31.768391	-1.858128	1.376320	0.006043	0.708008
-31.188490	-1.955814	1.381325	0.005935	0.708019
-31.498376	-1.905873	1.386330	0.005992	0.708009
-31.555876	-1.950798	1.391334	0.006003	0.707898
-32.419866	-1.896265	1.396339	0.006163	0.707699
-32.022088	-1.969086	1.401344	0.006089	0.707696
-32.300075	-1.914284	1.406349	0.006141	0.707706
-32.363268	-1.910014	1.411354	0.006153	0.707693
-32.244424	-1.926825	1.416358	0.006130	0.707701
-32.305069	-1.916979	1.421363	0.006142	0.707700
-32.616399	-1.942858	1.426368	0.006199	0.707537
-33.162234	-1.923543	1.431373	0.006301	0.707380
-33.138736	-1.932541	1.436378	0.006296	0.707371
-33.339199	-1.890701	1.441382	0.006334	0.707384
-33.368362	-1.889887	1.446387	0.006339	0.707375
-33.040581	-1.948096	1.451392	0.006278	0.707376
-33.115096	-1.933328	1.456397	0.006292	0.707379
-33.353826	-1.967907	1.461402	0.006336	0.707224
-33.990206	-1.923439	1.466406	0.006454	0.707086
-33.969726	-1.929138	1.471411	0.006450	0.707082
-34.181225	-1.891163	1.476416	0.006490	0.707083
-33.713534	-1.971276	1.481421	0.006403	0.707089
-33.704723	-1.976722	1.486426	0.006401	0.707082
-34.093758	-1.904115	1.491430	0.006473	0.707089
-34.479744	-1.985032	1.496435	0.006545	0.706788
-34.979792	-1.913929	1.501440	0.006638	0.706752
-34.887032	-1.925866	1.506445	0.006620	0.706762
-34.826345	-1.941721	1.511450	0.006609	0.706752
-34.759067	-1.949505	1.516454	0.006596	0.706760
-34.794901	-1.944934	1.521459	0.006603	0.706757
-34.930343	-1.933021	1.526464	0.006628	0.706733
-35.504423	-1.972725	1.531469	0.006735	0.706447
-35.985107	-1.889492	1.536474	0.006824	0.706443
-36.200206	-1.849360	1.541478	0.006864	0.706447
-35.744994	-1.932924	1.546483	0.006779	0.706442
-35.613788	-1.956802	1.551488	0.006755	0.706441
-35.846033	-1.911129	1.556493	0.006798	0.706450
-36.086839	-1.872783	1.561498	0.006843	0.706441
-35.936314	-2.017152	1.566502	0.006815	0.706205
-36.714381	-1.917399	1.571507	0.006959	0.706127
-36.989367	-1.868379	1.576512	0.007010	0.706127
-36.808746	-1.896601	1.581517	0.006977	0.706135
-36.771848	-1.909415	1.586522	0.006970	0.706123
-36.794937	-1.900826	1.591526	0.006974	0.706132
-36.713949	-1.916491	1.596531	0.006959	0.706130
-36.911216	-1.961884	1.601536	0.006995	0.705968
-37.591450	-1.889716	1.606541	0.007122	0.705870
-37.681434	-1.878090	1.611546	0.007138	0.705861
-37.393317	-1.927025	1.616550	0.007085	0.705866
-37.581790	-1.895052	1.621555	0.007120	0.705863
-37.874652	-1.843621	1.626560	0.007174	0.705862
-37.445531	-1.917260	1.631565	0.007094	0.705868
-37.532062	-2.016527	1.636570	0.007110	0.705637
-38.560928	-1.887002	1.641574	0.007302	0.705529
-38.382183	-1.922069	1.646579	0.007268	0.705523
-38.324993	-1.933221	1.651584	0.007257	0.705521
-38.369171	-1.922002	1.656589	0.007265	0.705528
-38.947718	-1.822403	1.661594	0.007373	0.705521
-38.617233	-1.878427	1.666598	0.007311	0.705527
-38.425392	-2.005116	1.671603	0.007276	0.705341
-39.814628	-1.820828	1.676608	0.007534	0.705214
-39.376278	-1.896739	1.681613	0.007452	0.705218
-39.276260	-1.919478	1.686618	0.007434	0.705209
-39.573600	-1.862943	1.691622	0.007489	0.705216
-39.609637	-1.858215	1.696627	0.007496	0.705213
-39.354916	-1.906435	1.701632	0.007448	0.705207
-39.112358	-2.008835	1.706637	0.007403	0.705088
-40.428774	-1.876472	1.711642	0.007648	0.704883
-40.153095	-1.919866	1.716646	0.007596	0.704894
-40.221955	-1.909790	1.721651	0.007609	0.704890
-40.493682	-1.863670	1.726656	0.007659	0.704886
-40.219752	-1.908147	1.731661	0.007608	0.704895
-40.153931	-1.925409	1.736666	0.007596	0.704884
-40.240977	-1.975655	1.741670	0.007612	0.704751
-41.216245	-1.879688	1.746675	0.007794	0.704595
-41.128143	-1.897898	1.751680	0.007777	0.704590
-41.091792	-1.900108	1.756685	0.007770	0.704599
-41.351983	-1.858599	1.761690	0.007819	0.704589
-40.929063	-1.931068	1.766694	0.007740	0.704595
-40.709378	-1.971222	1.771699	0.007699	0.704593
-41.352767	-1.956341	1.776704	0.007818	0.704392
-42.042947	-1.895277	1.781709	0.007947	0.704268
-41.800784	-1.942883	1.786714	0.007902	0.704259
-41.591781	-1.977573	1.791718	0.007863	0.704264
-42.230559	-1.864474	1.796723	0.007981	0.704263
-42.311935	-1.852281	1.801728	0.007996	0.704259
-41.627311	-1.970396	1.806733	0.007869	0.704267
-42.290256	-1.952984	1.811738	0.007992	0.704064
-43.382867	-1.811177	1.816742	0.008195	0.703957
-43.047822	-1.872514	1.821747	0.008133	0.703954
-43.333384	-1.822298	1.826752	0.008186	0.703953
-43.032715	-1.873020	1.831757	0.008130	0.703959
-42.854253	-1.908497	1.836762	0.008097	0.703952
-42.854322	-1.906888	1.841766	0.008097	0.703955
-43.076516	-1.869051	1.846771	0.008138	0.703952
-43.664764	-1.923372	1.851776	0.008247	0.703631
-43.507188	-1.947893	1.856781	0.008218	0.703638
-44.102606	-1.846424	1.861786	0.008328	0.703629
-43.890627	-1.881880	1.866790	0.008289	0.703634
-43.417195	-1.965877	1.871795	0.008201	0.703635
-43.844520	-1.891162	1.876800	0.008280	0.703632
-43.866399	-1.893283	1.881805	0.008284	0.703620
-44.570276	-1.909249	1.886810	0.008415	0.703335
-44.231816	-1.966752	1.891814	0.008352	0.703341
-44.585696	-1.904586	1.896819	0.008418	0.703339
-44.841098	-1.860478	1.901824	0.008465	0.703336
-44.554813	-1.907443	1.906829	0.008412	0.703345
-44.659138	-1.893667	1.911834	0.008431	0.703335
-44.575793	-1.944843	1.916838	0.008415	0.703262
-45.253177	-1.951547	1.921843	0.008541	0.703005
-45.508042	-1.908421	1.926848	0.008589	0.703001
-45.310086	-1.939953	1.931853	0.008552	0.703008
-45.616692	-1.890771	1.936858	0.008609	0.702997
-45.095641	-1.979320	1.941862	0.008512	0.703006
-45.369819	-1.932094	1.946867	0.008563	0.703003
-45.734223	-1.954302	1.951872	0.008630	0.702827
-46.275774	-1.922240	1.956877	0.008731	0.702697
-46.196032	-1.940577	1.961882	0.008716	0.702689
-46.373909	-1.907081	1.966886	0.008749	0.702693
-46.425005	-1.897267	1.971891	0.008759	0.702695
-46.174472	-1.944622	1.976896	0.008712	0.702689
-46.225595	-1.933761	1.981901	0.008721	0.702693
-46.970942	-1.924107	1.986906	0.008860	0.702444
-47.246880	-1.910259	1.991910	0.008911	0.702373
-46.765375	-1.997130	1.996915	0.008821	0.702371
-47.152773	-1.928237	2.001920	0.008893	0.702371

-47.225322	-1.916249	2.011917	0.008907	0.702370
-47.355200	-1.893345	2.021914	0.008931	0.702369
-48.013169	-1.898193	2.031910	0.009053	0.702123
-47.774449	-1.965105	2.041907	0.009008	0.702074
-48.212234	-1.875450	2.051904	0.009090	0.702098
-47.749811	-1.899806	2.061901	0.009003	0.702216
-47.263209	-1.912579	2.071898	0.008912	0.702366
-47.130594	-1.934771	2.081894	0.008887	0.702369
-47.161842	-1.928909	2.091891	0.008893	0.702370
-47.031865	-1.952446	2.101888	0.008869	0.702370
-47.020309	-1.955066	2.111885	0.008866	0.702369
-47.075090	-1.945588	2.121882	0.008876	0.702369
-47.106361	-1.940689	2.131878	0.008882	0.702368
-47.070450	-1.945949	2.141875	0.008875	0.702371
-46.903892	-1.976974	2.151872	0.008844	0.702369
-46.624165	-1.881915	2.161869	0.008791	0.702662
-46.440854	-1.901041	2.171866	0.008757	0.702690
-46.197769	-1.944124	2.181862	0.008712	0.702691
-46.171665	-1.948293	2.191859	0.008707	0.702692
-46.084328	-1.868874	2.201856	0.008690	0.702885
-45.514178	-1.913521	2.211853	0.008584	0.703000
-45.645372	-1.889920	2.221850	0.008608	0.703001
-45.451701	-1.923573	2.231846	0.008572	0.703003
-44.722335	-1.923852	2.241843	0.008436	0.703266
-44.833505	-1.867329	2.251840	0.008456	0.703340
-44.622263	-1.907286	2.261837	0.008416	0.703336
-44.861543	-1.844409	2.271834	0.008461	0.703377
-43.945612	-1.880233	2.281830	0.008290	0.703635
-43.787271	-1.909560	2.291827	0.008260	0.703633
-44.022178	-1.867897	2.301824	0.008304	0.703633
-43.234561	-1.904344	2.311821	0.008157	0.703844
-43.017253	-1.889919	2.321818	0.008116	0.703951
-43.004889	-1.892218	2.331814	0.008114	0.703951
-42.791759	-1.929956	2.341811	0.008074	0.703952
-42.276371	-1.870665	2.351808	0.007978	0.704258
-42.089261	-1.903454	2.361805	0.007943	0.704259
-42.044997	-1.911710	2.371802	0.007934	0.704259
-41.762521	-1.895922	2.381798	0.007881	0.704393
-41.118071	-1.911881	2.391795	0.007761	0.704593
-41.287904	-1.884107	2.401792	0.007792	0.704588
-41.135382	-1.909993	2.411789	0.007764	0.704591
-40.468795	-1.893447	2.421786	0.007640	0.704864
-40.315085	-1.908178	2.431782	0.007611	0.704890
-40.335134	-1.904700	2.441779	0.007614	0.704890
-40.223482	-1.854364	2.451776	0.007593	0.705032
-39.234923	-1.943277	2.461773	0.007409	0.705209
-39.510912	-1.895073	2.471770	0.007460	0.705207
-39.241942	-1.941983	2.481766	0.007410	0.705209
-38.921720	-1.873317	2.491763	0.007350	0.705463
-38.770323	-1.868949	2.501760	0.007321	0.705527
-38.750660	-1.873131	2.511757	0.007318	0.705526
-38.280479	-1.876533	2.521754	0.007230	0.705688
-37.585313	-1.914304	2.531750	0.007100	0.705862
-37.498050	-1.929524	2.541747	0.007084	0.705863
-37.675475	-1.897647	2.551744	0.007117	0.705864
-36.936861	-1.915005	2.561741	0.006979	0.706094
-36.990486	-1.891087	2.571738	0.006989	0.706123
-36.544487	-1.967717	2.581734	0.006905	0.706129
-36.957870	-1.832032	2.591731	0.006982	0.706255
-35.801564	-1.943825	2.601728	0.006767	0.706445
-36.180089	-1.876185	2.611725	0.006837	0.706445
-35.958085	-1.916079	2.621722	0.006795	0.706445
-35.244345	-1.888800	2.631718	0.006662	0.706756
-35.184742	-1.901773	2.641715	0.006651	0.706752
-35.013154	-1.931748	2.651712	0.006619	0.706753
-34.813592	-1.874316	2.661709	0.006581	0.706941
-34.388078	-1.881450	2.671706	0.006502	0.707079
-34.329913	-1.891015	2.681702	0.006491	0.707081
-34.422409	-1.833840	2.691699	0.006508	0.707163
-33.172603	-1.951099	2.701696	0.006275	0.707375
-33.480173	-1.896887	2.711693	0.006332	0.707375
-33.548076	-1.884686	2.721690	0.006344	0.707375
-32.770476	-1.894389	2.731686	0.006199	0.707634
-32.594270	-1.891921	2.741683	0.006166	0.707703
-32.346757	-1.935228	2.751680	0.006120	0.707705
-32.339796	-1.907699	2.761677	0.006118	0.707763
-31.771967	-1.885163	2.771674	0.006012	0.708011
-31.550780	-1.923154	2.781670	0.005971	0.708015
-31.743455	-1.887549	2.791667	0.006007	0.708018
-30.821607	-1.921970	2.801664	0.005835	0.708278
-30.860279	-1.878760	2.811661	0.005842	0.708352
-30.588716	-1.926233	2.821658	0.005791	0.708354
-30.538690	-1.926352	2.831654	0.005782	0.708372
-29.904890	-1.903208	2.841651	0.005663	0.708645
-29.755665	-1.930323	2.851648	0.005635	0.708644
-29.809370	-1.921042	2.861645	0.005645	0.708644
-29.648002	-1.870857	2.871642	0.005615	0.708803
-29.150065	-1.880823	2.881638	0.005522	0.708961
-29.074368	-1.893118	2.891635	0.005508	0.708964
-28.969730	-1.875603	2.901632	0.005488	0.709037
-28.353339	-1.870848	2.911629	0.005373	0.709267
-28.142456	-1.908402	2.921626	0.005333	0.709267
-28.102606	-1.914659	2.931622	0.005326	0.709269
-27.363728	-1.915636	2.941619	0.005188	0.709531
-27.201284	-1.910694	2.951616	0.005157	0.709599
-27.246732	-1.902417	2.961613	0.005166	0.709600
-27.039858	-1.921639	2.971610	0.005127	0.709636
-26.665991	-1.857699	2.981606	0.005057	0.709897
-26.340742	-1.916371	2.991603	0.004996	0.709896
-26.415706	-1.902717	3.001600	0.005010	0.709897
-26.000145	-1.849829	3.011597	0.004932	0.710152
-25.528294	-1.900453	3.021594	0.004844	0.710219
-25.557703	-1.895463	3.031590	0.004850	0.710219
-25.247029	-1.894061	3.041587	0.004792	0.710333
-24.553699	-1.916670	3.051584	0.004662	0.710535
-24.661418	-1.898393	3.061581	0.004682	0.710533
-24.540950	-1.919990	3.071578	0.004659	0.710534
-24.061435	-1.874383	3.081574	0.004570	0.710796
-23.690625	-1.901059	3.091571	0.004501	0.710875
-23.796157	-1.882624	3.101568	0.004520	0.710875
-23.614310	-1.889014	3.111565	0.004486	0.710927
-22.974227	-1.896875	3.121562	0.004367	0.711139
-22.902627	-1.909569	3.131558	0.004353	0.711140
-22.708464	-1.943159	3.141555	0.004317	0.711142
-22.315859	-1.892089	3.151552	0.004243	0.711384
-22.185955	-1.879647	3.161549	0.004219	0.711456
-21.978617	-1.916171	3.171546	0.004180	0.711457
-22.072048	-1.847640	3.181542	0.004197	0.711561
-21.017912	-1.934179	3.191539	0.004001	0.711763
-21.444436	-1.858480	3.201536	0.004080	0.711763
-21.159548	-1.909054	3.211533	0.004027	0.711764
-20.450173	-1.871104	3.221530	0.003894	0.712092
-20.267523	-1.903659	3.231526	0.003860	0.712092
-20.201496	-1.914417	3.241523	0.003848	0.712095
-20.161258	-1.844634	3.251520	0.003840	0.712249
-19.458662	-1.899147	3.261517	0.003709	0.712390
-19.610247	-1.872706	3.271514	0.003737	0.712389
-19.423689	-1.883129	3.281510	0.003702	0.712435
-18.585057	-1.892916	3.291507	0.003546	0.712713
-18.548757	-1.899358	3.301504	0.003539	0.712714
-18.261146	-1.950021	3.311501	0.003485	0.712715
-18.390848	-1.847499	3.321498	0.003509	0.712874
-17.586879	-1.914660	3.331494	0.003359	0.713026
-17.507691	-1.927054	3.341491	0.003344	0.713030
-17.647345	-1.903094	3.351488	0.003370	0.713028
-17.114815	-1.834895	3.361485	0.003270	0.713353
-16.590953	-1.923987	3.371482	0.003173	0.713362
-16.589419	-1.922429	3.381478	0.003172	0.713366
-16.512718	-1.869760	3.391475	0.003157	0.713499
-15.842710	-1.909131	3.401472	0.003033	0.713658
-15.697707	-1.934622	3.411469	0.003005	0.713659
-15.958155	-1.889735	3.421466	0.003054	0.713657
-15.311097	-1.876376	3.431462	0.002933	0.713913
-15.141001	-1.874415	3.441459	0.002901	0.713977
-15.034054	-1.893676	3.451456	0.002881	0.713977
-14.802841	-1.865560	3.461453	0.002838	0.714115
-14.186606	-1.891617	3.471450	0.002723	0.714282
-14.320166	-1.866858	3.481446	0.002747	0.714285
-14.037168	-1.916731	3.491443	0.002694	0.714286
-13.400792	-1.864869	3.501440	0.002576	0.714615
-13.013204	-1.934943	3.511437	0.002503	0.714613
-13.339070	-1.876875	3.521434	0.002564	0.714614
-12.993215	-1.884658	3.531430	0.002499	0.714721
-12.448721	-1.883410	3.541427	0.002397	0.714916
-12.344603	-1.901615	3.551424	0.002378	0.714917
-12.438305	-1.886751	3.561421	0.002395	0.714914
-11.610446	-1.883173	3.571418	0.002241	0.715214
-11.587381	-1.875125	3.581414	0.002236	0.715239
-11.655776	-1.863233	3.591411	0.002249	0.715239
-11.282014	-1.849029	3.601408	0.002179	0.715399
-10.521197	-1.908313	3.611405	0.002037	0.715551
-10.741407	-1.869579	3.621402	0.002078	0.715550
-10.291188	-1.948835	3.631398	0.001994	0.715553
-9.791764	-1.896310	3.641395	0.001901	0.715834
-9.312314	-1.953844	3.651392	0.001811	0.715889
-9.422056	-1.934944	3.661389	0.001831	0.715888
-9.411414	-1.936932	3.671386	0.001829	0.715889
-8.808084	-1.932103	3.681382	0.001717	0.716112
-8.762583	-1.926221	3.691379	0.001708	0.716140
-8.635172	-1.950583	3.701376	0.001684	0.716137
-8.627873	-1.891118	3.711373	0.001682	0.716258
-7.562642	-1.983365	3.721370	0.001484	0.716451
-7.672653	-1.963944	3.731366	0.001504	0.716451
-7.799036	-1.940779	3.741363	0.001527	0.716453
-7.204632	-1.948195	3.751360	0.001416	0.716648
-6.873730	-1.949513	3.761357	0.001355	0.716763
-6.738057	-1.975979	3.771354	0.001329	0.716759
-6.923190	-1.943732	3.781350	0.001363	0.716758
-6.130303	-1.917265	3.791347	0.001215	0.717090
-5.632535	-2.005886	3.801344	0.001123	0.717090
-5.897347	-1.960201	3.811341	0.001172	0.717088
-5.869010	-1.930308	3.821338	0.001166	0.717158
-4.998229	-1.971388	3.831334	0.001004	0.717383
-4.809406	-2.003369	3.841331	0.000968	0.717387
-4.890300	-1.989490	3.851328	0.000983	0.717387
-4.505330	-1.967135	3.861325	0.000911	0.717567
-4.079847	-1.971656	3.871322	0.000832	0.717708
-3.984314	-1.987614	3.881318	0.000814	0.717711
-3.966358	-1.990707	3.891315	0.000810	0.717711
-3.173441	-1.993739	3.901312	0.000663	0.717985
-3.084899	-1.990854	3.911309	0.000646	0.718022
-2.855161	-2.033044	3.921306	0.000603	0.718020
-3.101156	-1.980433	3.931302	0.000648	0.718038
-2.307106	-1.957880	3.941299	0.000500	0.718362
-2.315691	-1.955415	3.951296	0.000502	0.718364
-2.304220	-1.960082	3.961293	0.000499	0.718359
-2.007557	-1.935403	3.971290	0.000444	0.718513
-1.839048	-1.897228	3.981286	0.000412	0.718648
-1.777746	-1.907128	3.991283	0.000401	0.718650
-1.635779	-1.854829	4.001280	0.000374	0.718804
-1.623319	-1.774146	4.011277	0.000371	0.718968
-1.385150	-1.816450	4.021274	0.000327	0.718969
-1.572171	-1.646315	4.031270	0.000361	0.719239
-1.448931	-1.648463	4.041267	0.000338	0.719279
-0.974851	-1.621507	4.051264	0.000250	0.719499
-1.057407	-1.550500	4.061261	0.000265	0.719610
-1.147513	-1.456020	4.071258	0.000281	0.719765
-0.788789	-1.447228	4.081254	0.000214	0.719909
-0.981508	-1.312352	4.091251	0.000250	0.720107
-0.907546	-1.262263	4.101248	0.000236	0.720232
-0.759270	-1.145752	4.111245	0.000208	0.720514
-0.747192	-1.087467	4.121242	0.000205	0.720634
-0.721642	-0.965702	4.131238	0.000200	0.720883
-0.714986	-0.871590	4.141235	0.000199	0.721071
-0.440630	-0.842196	4.151232	0.000147	0.721225
-0.612201	-0.698545	4.161229	0.000179	0.721448
-0.284512	-0.612140	4.171226	0.000118	0.721733
-0.319820	-0.497360	4.181222	0.000124	0.721947
-0.215175	-0.398116	4.191219	0.000104	0.722179
-0.115848	-0.302224	4.201216	0.000085	0.722402
-0.092491	-0.154956	4.211213	0.000081	0.722700
-0.211080	0.007010	4.221210	0.000103	0.722977
0.000000	0.125643	4.231206	0.000063	0.723284

-0.005154	0.761560	4.236211	0.000063	0.724528
-0.019899	2.037204	4.241216	0.000065	0.727017
0.420747	3.821201	4.246221	-0.000018	0.730643
0.893840	6.160881	4.251226	-0.000108	0.735335
1.257472	9.030599	4.256230	-0.000178	0.740975
1.669384	12.371844	4.261235	-0.000257	0.747484
2.147365	16.158603	4.266240	-0.000348	0.754797
2.596807	20.351010	4.271245	-0.000435	0.762785
3.018032	24.956343	4.276250	-0.000516	0.771440
3.391726	29.932734	4.281254	-0.000589	0.780659
3.884939	35.233079	4.286259	-0.000685	0.790389
4.525514	40.834719	4.291264	-0.000808	0.800581
6.029273	46.579802	4.296269	-0.001091	0.811163
8.762894	52.430851	4.301274	-0.001604	0.822166
9.303269	58.966425	4.306278	-0.001709	0.833527
9.869116	65.697780	4.311283	-0.001819	0.845073
11.703666	72.457918	4.316288	-0.002165	0.856880
12.763825	79.567469	4.321293	-0.002367	0.868873
13.819268	86.869678	4.326298	-0.002569	0.881011
15.093283	94.310720	4.331302	-0.002811	0.893265
15.498509	102.038185	4.336307	-0.002892	0.905563
16.371603	109.842672	4.341312	-0.003059	0.917941
17.294575	117.738006	4.346317	-0.003236	0.930305
18.553477	125.701916	4.351322	-0.003476	0.942699
19.559386	133.833144	4.356326	-0.003669	0.955113
20.175168	142.092766	4.361331	-0.003789	0.967456
21.063518	150.404771	4.366336	-0.003960	0.979788
22.016974	158.783306	4.371341	-0.004143	0.992078
22.714633	167.237439	4.376346	-0.004279	1.004260
23.504619	175.726911	4.381350	-0.004431	1.016367
24.170692	184.259632	4.386355	-0.004561	1.028362
25.124096	192.799043	4.391360	-0.004744	1.040295
25.516959	201.451713	4.396365	-0.004823	1.052113
26.314397	210.051942	4.401370	-0.004977	1.063824
27.249717	218.673942	4.406374	-0.005157	1.075467
27.658783	227.347553	4.411379	-0.005239	1.086933
28.426152	235.995502	4.416384	-0.005388	1.098326
29.319287	244.610235	4.421389	-0.005560	1.109587
29.905722	253.285842	4.426394	-0.005675	1.120744
30.824528	261.900916	4.431398	-0.005852	1.131787
31.477319	270.557067	4.436403	-0.005979	1.142717
32.003731	279.276595	4.441408	-0.006083	1.153594
32.659883	287.897063	4.446413	-0.006211	1.164276
33.156009	296.552980	4.451418	-0.006309	1.174870
34.145420	305.104222	4.456422	-0.006499	1.185345
34.662906	313.737990	4.461427	-0.006601	1.195730
35.645252	322.263310	4.466432	-0.006789	1.205991
36.328262	330.854364	4.471437	-0.006922	1.216182
36.775914	339.460997	4.476442	-0.007011	1.226260
37.547498	348.031987	4.481446	-0.007161	1.236277
38.106379	356.565512	4.486451	-0.007270	1.246130
39.064351	365.066521	4.491456	-0.007454	1.255945
39.519185	373.612094	4.496461	-0.007545	1.265638
40.106512	382.144032	4.501466	-0.007660	1.275267
40.670417	390.638818	4.506470	-0.007770	1.284778
41.000254	399.162340	4.511475	-0.007838	1.294207
41.742436	407.606490	4.516480	-0.007981	1.303557
42.169040	416.183364	4.521485	-0.008066	1.312926
42.689636	424.644676	4.526490	-0.008169	1.322122
43.583242	433.006036	4.531494	-0.008341	1.331214
44.126784	441.414110	4.536499	-0.008448	1.340231
44.837569	449.800537	4.541504	-0.008586	1.349194
45.335898	458.209740	4.546509	-0.008684	1.358085
46.048601	466.560198	4.551514	-0.008822	1.366894
46.924484	474.917218	4.556518	-0.008991	1.375681
47.277524	483.314051	4.561523	-0.009062	1.384363
47.839968	491.707103	4.566528	-0.009173	1.393023
48.096638	500.091723	4.571533	-0.009226	1.401569
48.868353	508.390592	4.576538	-0.009375	1.410063
49.300716	516.757244	4.581542	-0.009461	1.418517
49.859569	525.068449	4.586547	-0.009571	1.426886
50.339655	533.433305	4.591552	-0.009666	1.435247
50.787001	541.741768	4.596557	-0.009755	1.443499
51.254212	550.067064	4.601562	-0.009847	1.451723
51.998651	558.349090	4.606566	-0.009991	1.459902
52.310133	566.678179	4.611571	-0.010055	1.468013
52.778037	575.043012	4.616576	-0.010147	1.476138
53.313461	583.290863	4.621581	-0.010253	1.484117
53.833806	591.566452	4.626586	-0.010355	1.492077
54.516684	599.798319	4.631590	-0.010488	1.499978
54.832749	608.087486	4.636595	-0.010552	1.507836
55.551364	616.330118	4.641600	-0.010691	1.515670
56.173198	624.560773	4.646605	-0.010813	1.523438
56.631654	632.834835	4.651610	-0.010903	1.531182
57.317387	641.077258	4.656614	-0.011037	1.538892
57.861519	649.323347	4.661619	-0.011143	1.546545
58.369339	657.609696	4.666624	-0.011244	1.554192
58.836354	665.835712	4.671629	-0.011336	1.561740
59.774298	673.996060	4.676634	-0.011516	1.569261
60.352044	682.248884	4.681638	-0.011629	1.576777
60.820772	690.473836	4.686643	-0.011722	1.584217
61.213908	698.737059	4.691648	-0.011801	1.591644
61.477517	706.993591	4.696653	-0.011855	1.599013
61.941261	715.201599	4.701658	-0.011947	1.606333
62.761883	723.393500	4.706662	-0.012105	1.613656
63.004392	731.630517	4.711667	-0.012156	1.620905
63.469643	739.860893	4.716672	-0.012248	1.628146
63.939200	748.127619	4.721677	-0.012341	1.635387
64.344714	756.310887	4.726682	-0.012422	1.642515
64.611280	764.534682	4.731686	-0.012477	1.649627
64.937666	772.740803	4.736691	-0.012543	1.656703
65.476114	780.907851	4.741696	-0.012649	1.663743
65.792850	789.112871	4.746701	-0.012713	1.670756
65.932982	797.333198	4.751706	-0.012745	1.677729
66.513579	805.474995	4.756710	-0.012858	1.684665
67.419056	813.562589	4.761715	-0.013032	1.691571
67.908753	821.763860	4.766720	-0.013129	1.698488
68.265709	829.941091	4.771725	-0.013201	1.705339
68.789660	838.135160	4.776730	-0.013304	1.712199
69.290860	846.309978	4.781734	-0.013403	1.719012
69.738330	854.448228	4.786739	-0.013491	1.725762
70.378614	862.625467	4.791744	-0.013616	1.732541
71.000463	870.766806	4.796749	-0.013737	1.739262
71.002585	878.995630	4.801754	-0.013743	1.745950
71.487898	887.160118	4.806758	-0.013839	1.752621
72.228708	895.265582	4.811763	-0.013982	1.759251
72.727558	903.423147	4.816768	-0.014081	1.765867
73.122066	911.603059	4.821773	-0.014159	1.772464
73.541227	919.766109	4.826778	-0.014243	1.779025
74.141613	927.894424	4.831782	-0.014360	1.785557
74.555949	936.101906	4.836787	-0.014443	1.792105
74.949482	944.279811	4.841792	-0.014521	1.798603
75.531581	952.368814	4.846797	-0.014635	1.805031
75.974709	960.527461	4.851802	-0.014723	1.811473
76.537572	968.668893	4.856806	-0.014833	1.817893
76.768894	976.823740	4.861811	-0.014882	1.824261
77.210845	984.976362	4.866816	-0.014970	1.830631
77.474720	993.149321	4.871821	-0.015024	1.836972
78.123051	1001.239413	4.876826	-0.015150	1.843274
78.516359	1009.393616	4.881830	-0.015229	1.849573
78.543667	1017.584111	4.886835	-0.015239	1.855835
79.025575	1025.705582	4.891840	-0.015335	1.862077
79.477043	1033.826253	4.896845	-0.015424	1.868293
79.897189	1041.986831	4.901850	-0.015508	1.874516
80.401925	1050.079326	4.906854	-0.015607	1.880676
80.748616	1058.191646	4.911859	-0.015677	1.886812
81.076598	1066.355470	4.916864	-0.015744	1.892965
81.295357	1074.500959	4.921869	-0.015790	1.899072
81.848816	1082.574756	4.926874	-0.015898	1.905144
82.404599	1090.699130	4.931878	-0.016007	1.911234
82.593583	1098.860064	4.936883	-0.016048	1.917290
83.100422	1106.948601	4.941888	-0.016147	1.923310
83.725241	1115.034759	4.946893	-0.016269	1.929322
83.945456	1123.198581	4.951898	-0.016316	1.935327
84.216320	1131.337557	4.956902	-0.016371	1.941301
84.424957	1139.467390	4.961907	-0.016416	1.947243
84.991107	1147.616318	4.966912	-0.016526	1.953219
85.218705	1155.740461	4.971917	-0.016574	1.959123
85.556320	1163.811137	4.976922	-0.016642	1.964982
86.151470	1171.896918	4.981926	-0.016759	1.970862
86.286170	1180.033677	4.986931	-0.016789	1.976712
86.683192	1188.141002	4.991936	-0.016868	1.982552
87.081161	1196.236045	4.996941	-0.016948	1.988365
87.365177	1204.371381	5.001946	-0.017006	1.994178
87.961743	1212.438306	5.006950	-0.017123	1.999959
88.284642	1220.521803	5.011955	-0.017188	2.005705
88.673351	1228.657644	5.016960	-0.017266	2.011479
89.119720	1236.760418	5.021965	-0.017355	2.017219
89.609466	1244.843231	5.026970	-0.017451	2.022933
90.194611	1252.939528	5.031974	-0.017565	2.028650
90.443123	1261.102583	5.036979	-0.017617	2.034363
90.867976	1269.186874	5.041984	-0.017702	2.040023
91.178547	1277.276437	5.046989	-0.017765	2.045659
91.506277	1285.384938	5.051994	-0.017831	2.051295
91.656900	1293.525122	5.056998	-0.017865	2.056919
92.071960	1301.582013	5.062003	-0.017947	2.062497
92.480184	1309.675517	5.067008	-0.018029	2.068084
92.621987	1317.828211	5.072013	-0.018061	2.073670
92.979182	1325.894188	5.077018	-0.018132	2.079203
93.408604	1333.968014	5.082022	-0.018218	2.084734
93.814598	1342.049510	5.087027	-0.018299	2.090253
94.156915	1350.176485	5.092032	-0.018368	2.095781
94.461868	1358.258064	5.097037	-0.018430	2.101261
94.813875	1366.346530	5.102042	-0.018501	2.106736
95.226991	1374.487356	5.107046	-0.018583	2.112237
95.377216	1382.612151	5.112051	-0.018617	2.117688
96.063715	1390.630075	5.117056	-0.018750	2.123106
96.317054	1398.727701	5.122061	-0.018802	2.128520
96.686859	1406.813449	5.127066	-0.018877	2.133924
96.973629	1414.923626	5.132070	-0.018935	2.139323
97.355633	1422.973005	5.137075	-0.019012	2.144677
97.413769	1431.115145	5.142080	-0.019028	2.150048
97.816094	1439.182017	5.147085	-0.019108	2.155389
98.149028	1447.253831	5.152090	-0.019176	2.160713
98.414490	1455.342034	5.157094	-0.019231	2.166028
98.647283	1463.430287	5.162099	-0.019279	2.171327
99.205398	1471.490908	5.167104	-0.019389	2.176625
99.610526	1479.567271	5.172109	-0.019469	2.181907
99.808079	1487.667540	5.177114	-0.019512	2.187172
100.649011	1495.722745	5.182118	-0.019674	2.192453
100.986169	1503.806023	5.187123	-0.019742	2.197695
101.486695	1511.873943	5.192128	-0.019840	2.202928
101.891118	1519.951317	5.197133	-0.019921	2.208147
102.271934	1528.050203	5.202138	-0.019997	2.213364
102.987414	1536.101978	5.207142	-0.020136	2.218569
103.261673	1544.182483	5.212147	-0.020192	2.223741
103.636268	1552.282736	5.217152	-0.020267	2.228922
103.815101	1560.402099	5.222157	-0.020306	2.234086
104.058837	1568.481188	5.227162	-0.020357	2.239218
104.362164	1576.548416	5.232166	-0.020419	2.244336
104.568727	1584.630620	5.237171	-0.020463	2.249443
104.957393	1592.731939	5.242176	-0.020540	2.254567
105.211389	1600.791615	5.247181	-0.020593	2.259641
105.515769	1608.855379	5.252186	-0.020655	2.264711
105.996264	1616.942642	5.257190	-0.020750	2.269798
106.375439	1625.083479	5.262195	-0.020826	2.274899
106.876322	1633.101565	5.267200	-0.020925	2.279923
107.292427	1641.146093	5.272205	-0.021007	2.284945
107.318220	1649.247621	5.277210	-0.021018	2.289958
107.689944	1657.337174	5.282214	-0.021092	2.294981
108.024169	1665.369666	5.287219	-0.021160	2.299956
108.411525	1673.439226	5.292224	-0.021237	2.304946
108.781142	1681.511394	5.297229	-0.021311	2.309926
108.835344	1689.611857	5.302234	-0.021327	2.314886
109.093115	1697.685618	5.307238	-0.021380	2.319836
109.461856	1705.720153	5.312243	-0.021454	2.324761
109.706131	1713.791217	5.317248	-0.021505	2.329687
109.973690	1721.886691	5.322253	-0.021560	2.334620
110.278701	1729.944062	5.327258	-0.021622	2.339522
110.610113	1738.018603	5.332262	-0.021690	2.344426
110.918730	1746.067739	5.337267	-0.021752	2.349303
111.510625	1754.155361	5.342272	-0.021868	2.354215
111.752797	1762.217320	5.347277	-0.021918	2.359074
112.079780	1770.262233	5.352282	-0.021985	2.363919
112.491794	1778.328408	5.357286	-0.022067	2.368774
112.638544	1786.415035	5.362291	-0.022099	2.373610
113.225585	1794.448806	5.367296	-0.022214	2.378439
113.419355	1802.537165	5.372301	-0.022256	2.383260
113.525147	1810.619262	5.377306	-0.022281	2.388060
114.084433	1818.689728	5.382310	-0.022390	2.392879
114.429036	1826.734244	5.387315	-0.022460	2.397657
114.774743	1834.799935	5.392320	-0.022529	2.402437
114.828199	1842.883525	5.397325	-0.022545	2.407196
115.327719	1850.941080	5.402330	-0.022643	2.411964
115.799226	1859.011959	5.407334	-0.022736	2.416729
115.886067	1867.074280	5.412339	-0.022758	2.421449
116.390140	1875.114760	5.417344	-0.022857	2.426180
116.726320	1883.193122	5.422349	-0.022925	2.430910
116.662375	1891.349491	5.427354	-0.022919	2.435646
117.141928	1899.359552	5.432358	-0.023013	2.440330
117.431953	1907.361061	5.437363	-0.023072	2.444985
117.655835	1915.439132	5.442368	-0.023120	2.449670
118.277152	1923.470294	5.447373	-0.023241	2.454349
118.737344	1931.503215	5.452378	-0.023332	2.459008
118.995757	1939.580700	5.457382	-0.023385	2.463668
118.944046	1947.673426	5.462387	-0.023381	2.468306
119.432022	1955.732230	5.467392	-0.023477	2.472955
119.962887	1963.760210	5.472397	-0.023581	2.477581
119.990634	1971.830918	5.477402	-0.023592	2.482185
120.412727	1979.880722	5.482406	-0.023676	2.486799
120.684330	1987.939615	5.487411	-0.023732	2.491397
120.882724	1996.039278	5.492416	-0.023774	2.496005
121.224562	2004.083955	5.497421	-0.023843	2.500583
121.673294	2012.086441	5.502426	-0.023932	2.505138
122.159811	2020.165145	5.507430	-0.024028	2.509729
122.339263	2028.276116	5.512435	-0.024067	2.514308
122.588459	2036.337180	5.517440	-0.024118	2.518855
122.913655	2044.338919	5.522445	-0.024184	2.523367
123.318992	2052.389057	5.527450	-0.024265	2.527903
123.621146	2060.462030	5.532454	-0.024327	2.532436
123.757460	2068.543875	5.537459	-0.024358	2.536954
124.023482	2076.584190	5.542464	-0.024412	2.541451
124.343106	2084.621161	5.547469	-0.024477	2.545941
124.671774	2092.678704	5.552474	-0.024544	2.550435
124.905003	2100.780788	5.557478	-0.024593	2.554940
125.189064	2108.802186	5.562483	-0.024651	2.559395
125.739928	2116.812617	5.567488	-0.024759	2.563855
125.997994	2124.884389	5.572493	-0.024812	2.568320
126.254591	2132.956645	5.577498	-0.024865	2.572778
126.568716	2141.033862	5.582502	-0.024929	2.577235
126.954535	2149.061560	5.587507	-0.025006	2.581662
127.370705	2157.104341	5.592512	-0.025089	2.586091
127.745633	2165.178621	5.597517	-0.025164	2.590528
128.118055	2173.403958	5.602522	-0.025239	2.595038
128.777069	2181.364805	5.607526	-0.025367	2.599417
128.992990	2189.363191	5.612531	-0.025413	2.603778
129.109989	2197.409281	5.617536	-0.025440	2.608151
129.534829	2205.437756	5.622541	-0.025524	2.612528
129.857730	2213.466270	5.627546	-0.025590	2.616891
130.113830	2221.538338	5.632550	-0.025643	2.621265
130.206701	2229.558358	5.637555	-0.025666	2.625593
130.603685	2237.610880	5.642560	-0.025745	2.629952
130.905251	2245.691058	5.647565	-0.025806	2.634312
131.081042	2253.721282	5.652570	-0.025844	2.638629
131.447169	2261.772690	5.657574	-0.025918	2.642963
131.587645	2269.803160	5.662579	-0.025949	2.647265
131.950070	2277.860681	5.667584	-0.026022	2.651588
132.218543	2285.941854	5.672589	-0.026078	2.655910
132.485337	2293.960189	5.677594	-0.026133	2.660192
132.893861	2302.005582	5.682598	-0.026214	2.664490
133.097755	2310.064278	5.687603	-0.026257	2.668776
133.278296	2318.167220	5.692608	-0.026296	2.673076
133.538356	2326.215767	5.697613	-0.026350	2.677345
133.889813	2334.207070	5.702618	-0.026421	2.681584
134.407301	2342.228595	5.707622	-0.026523	2.685842
134.702022	2350.273324	5.712627	-0.026583	2.690091
134.882761	2358.372015	5.717632	-0.026622	2.694355
135.113987	2366.425148	5.722637	-0.026670	2.698591
135.023719	2374.471059	5.727642	-0.026659	2.702797
135.354636	2382.518586	5.732646	-0.026726	2.707023
135.719383	2390.541321	5.737651	-0.026799	2.711232
135.941212	2398.610558	5.742656	-0.026846	2.715450
136.161183	2406.630828	5.747661	-0.026892	2.719635
136.337542	2414.671173	5.752666	-0.026930	2.723821
136.557403	2422.733905	5.757670	-0.026977	2.728016
136.691415	2430.803650	5.762675	-0.027007	2.732202
136.895052	2438.868567	5.767680	-0.027050	2.736384
137.405034	2446.871079	5.772685	-0.027150	2.740545
137.612960	2454.882212	5.777690	-0.027194	2.744687
137.927418	2462.987768	5.782694	-0.027258	2.748877
138.104372	2471.078840	5.787699	-0.027297	2.753045
138.540956	2479.131165	5.792704	-0.027383	2.757202
138.846100	2487.131980	5.797709	-0.027446	2.761319
138.969663	2495.140458	5.802714	-0.027474	2.765422
139.362770	2503.166813	5.807718	-0.027552	2.769545
139.729352	2511.230501	5.812723	-0.027626	2.773679
139.850638	2519.294431	5.817728	-0.027654	2.777792
140.334800	2527.290213	5.822733	-0.027749	2.781886
140.653896	2535.301778	5.827738	-0.027814	2.785972
140.888217	2543.376383	5.832742	-0.027863	2.790079
141.081174	2551.449899	5.837747	-0.027905	2.794177
141.558957	2559.467966	5.842752	-0.027999	2.798257
141.807182	2567.499643	5.847757	-0.028050	2.802325
141.695714	2575.573264	5.852762	-0.028035	2.806388
142.222138	2583.597857	5.857766	-0.028138	2.810456
142.478569	2591.668994	5.862771	-0.028191	2.814527
142.736033	2599.707019	5.867776	-0.028245	2.818575
142.944850	2607.747955	5.872781	-0.028289	2.822615
143.272952	2615.750122	5.877786	-0.028355	2.826638
143.651032	2623.825737	5.882790	-0.028431	2.830694
143.843031	2631.899813	5.887795	-0.028472	2.834733
144.229103	2639.903972	5.892800	-0.028550	2.838742
144.719502	2647.917928	5.897805	-0.028646	2.842756
144.662085	2655.971954	5.902810	-0.028641	2.846754
145.100759	2664.022352	5.907814	-0.028728	2.850772
145.198962	2672.090466	5.912819	-0.028752	2.854774
145.388852	2680.108517	5.917824	-0.028792	2.858751
145.712212	2688.144398	5.922829	-0.028858	2.862738
146.199777	2696.141007	5.927834	-0.028954	2.866710
146.900184	2704.180403	5.932838	-0.029090	2.870709
146.978699	2712.256236	5.937843	-0.029110	2.874685
147.278425	2720.277994	5.942848	-0.029171	2.878642
147.569319	2728.319584	5.947853	-0.029230	2.882603
147.867005	2736.344225	5.952858	-0.029291	2.886550
148.339526	2744.387500	5.957862	-0.029384	2.890510
148.696495	2752.454194	5.962867	-0.029456	2.894470
148.889203	2760.505418	5.967872	-0.029498	2.898408
149.214222	2768.531342	5.972877	-0.029563	2.902336
149.362176	2776.569791	5.977882	-0.029596	2.906254
149.805082	2784.604841	5.982886	-0.029684	2.910182
150.032810	2792.762760	5.987891	-0.029732	2.914152
150.359045	2800.744506	5.992896	-0.029798	2.918037
150.513640	2808.786781	5.997901	-0.029832	2.921937
150.789379	2816.771751	6.002906	-0.029889	2.925810
150.846220	2824.827496	6.007910	-0.029905	2.929700
151.122798	2832.872097	6.012915	-0.029962	2.933592
151.520276	2840.888485	6.017920	-0.030041	2.937471
151.823436	2848.943432	6.022925	-0.030103	2.941359
151.977919	2856.950403	6.027930	-0.030137	2.945210
152.347466	2865.001481	6.032934	-0.030211	2.949089
152.351596	2873.068058	6.037939	-0.030217	2.952951
152.662912	2881.105714	6.042944	-0.030280	2.956810
152.906640	2889.127263	6.047949	-0.030331	2.960653
153.110717	2897.141337	6.052954	-0.030374	2.964485
153.515359	2905.180575	6.057958	-0.030455	2.968335
153.507852	2913.237585	6.062963	-0.030459	2.972167
153.739113	2921.288164	6.067968	-0.030508	2.976003
154.126525	2929.302401	6.072973	-0.030585	2.979824
154.475253	2937.321347	6.077978	-0.030655	2.983641
154.773083	2945.371979	6.082982	-0.030716	2.987466
154.822274	2953.450074	6.087987	-0.030731	2.991286
155.224058	2961.490142	6.092992	-0.030811	2.995101
155.487728	2969.498867	6.097997	-0.030865	2.998889
155.741895	2977.479711	6.103002	-0.030918	3.002659
155.855321	2985.551243	6.108006	-0.030944	3.006460
156.185409	2993.558517	6.113011	-0.031011	3.010236
156.444183	3001.641418	6.118016	-0.031065	3.014039
156.832195	3009.656522	6.123021	-0.031142	3.017813
157.003546	3017.683019	6.128026	-0.031180	3.021576
157.213898	3025.734295	6.133030	-0.031224	3.025348
157.464103	3033.746756	6.138035	-0.031276	3.029099
157.625948	3041.832043	6.143040	-0.031311	3.032875
157.914847	3049.896944	6.148045	-0.031371	3.036643
158.020559	3057.882024	6.153050	-0.031396	3.040360
158.292596	3065.914341	6.158054	-0.031452	3.044103
158.435412	3073.942329	6.163059	-0.031484	3.047833
158.748347	3081.989120	6.168064	-0.031547	3.051575
158.982537	3090.048603	6.173069	-0.031596	3.055314
159.135843	3098.054670	6.178074	-0.031630	3.059021
159.493112	3106.080913	6.183078	-0.031702	3.062742
159.612770	3114.141923	6.188083	-0.031730	3.066463
159.850734	3122.160086	6.193088	-0.031779	3.070165
160.163672	3130.284420	6.198093	-0.031843	3.073915
160.443381	3138.284114	6.203098	-0.031900	3.077602
160.630532	3146.298795	6.208102	-0.031940	3.081287
160.943090	3154.269645	6.213107	-0.032004	3.084953
161.351068	3162.302688	6.218112	-0.032085	3.088648
161.595842	3170.358504	6.223117	-0.032136	3.092341
161.639580	3178.426396	6.228122	-0.032150	3.096026
162.079683	3186.431481	6.233126	-0.032237	3.099696
162.245975	3194.455040	6.238131	-0.032273	3.103357
162.423969	3202.495932	6.243136	-0.032312	3.107023
162.890036	3210.552903	6.248141	-0.032404	3.110704
163.048078	3218.568246	6.253146	-0.032439	3.114348
163.167852	3226.611320	6.258150	-0.032466	3.117999
163.297943	3234.655972	6.263155	-0.032496	3.121647
163.686998	3242.661128	6.268160	-0.032574	3.125284
163.913484	3250.680027	6.273165	-0.032621	3.128916
164.028366	3258.743543	6.278170	-0.032648	3.132559
164.463461	3266.779634	6.283174	-0.032734	3.136199
164.438773	3274.801474	6.288179	-0.032735	3.139808
164.717399	3282.811319	6.293184	-0.032792	3.143421
165.183456	3290.841518	6.298189	-0.032884	3.147048
165.202592	3298.902311	6.303194	-0.032893	3.150664
165.588857	3306.956347	6.308198	-0.032971	3.154289
165.797006	3314.970749	6.313203	-0.033015	3.157884
166.131077	3322.978056	6.318208	-0.033082	3.161478
166.416023	3330.986084	6.323213	-0.033141	3.165065
166.499965	3339.004447	6.328218	-0.033162	3.168644
166.887939	3347.093943	6.333222	-0.033239	3.172264
166.986945	3355.120132	6.338227	-0.033263	3.175840
167.242791	3363.137636	6.343232	-0.033316	3.179414
167.564122	3371.169316	6.348237	-0.033381	3.182993
167.950741	3379.174408	6.353242	-0.033458	3.186559
168.282741	3387.238283	6.358246	-0.033526	3.190144
168.393309	3395.276593	6.363251	-0.033552	3.193705
168.670907	3403.340669	6.368256	-0.033609	3.197281
168.935146	3411.359273	6.373261	-0.033663	3.200831
169.046569	3419.321956	6.378266	-0.033689	3.204347
169.380547	3427.404461	6.383270	-0.033757	3.207921
169.716551	3435.435612	6.388275	-0.033825	3.211468
169.811223	3443.479904	6.393280	-0.033848	3.215007
170.087647	3451.512596	6.398285	-0.033904	3.218545
170.314024	3459.502653	6.403290	-0.033952	3.222058
170.517815	3467.523616	6.408294	-0.033995	3.225579
170.771517	3475.580952	6.413299	-0.034048	3.229115
171.170211	3483.635265	6.418304	-0.034127	3.232651
171.372564	3491.730327	6.423309	-0.034171	3.236193
171.461483	3499.677920	6.428314	-0.034192	3.239663
171.746820	3507.712829	6.433318	-0.034251	3.243174
172.031935	3515.728618	6.438323	-0.034309	3.246674
172.009940	3523.744669	6.443328	-0.034310	3.250157
172.360482	3531.806505	6.448333	-0.034381	3.253672
172.493362	3539.828661	6.453338	-0.034411	3.257157
172.786263	3547.850693	6.458342	-0.034471	3.260644
172.894809	3555.879432	6.463347	-0.034497	3.264123
173.383792	3563.875118	6.468352	-0.034593	3.267599
173.764720	3571.934173	6.473357	-0.034669	3.271095
173.851321	3579.971382	6.478362	-0.034691	3.274565
174.036761	3588.022047	6.483366	-0.034731	3.278042
174.296870	3596.030391	6.488371	-0.034784	3.281500
174.578115	3604.010556	6.493376	-0.034842	3.284942
174.903301	3612.086202	6.498381	-0.034908	3.288424
175.209139	3620.116977	6.503386	-0.034970	3.291882
175.295243	3628.176636	6.508390	-0.034992	3.295340
175.450421	3636.186886	6.513395	-0.035026	3.298776
175.595312	3644.213054	6.518400	-0.035058	3.302215
175.931437	3652.224912	6.523405	-0.035126	3.305651
176.034322	3660.257802	6.528410	-0.035151	3.309084
176.275809	3668.305938	6.533414	-0.035201	3.312525
176.539686	3676.364268	6.538419	-0.035255	3.315968
176.773198	3684.344215	6.543424	-0.035304	3.319373
176.969915	3692.384188	6.548429	-0.035346	3.322798
176.982832	3700.402987	6.553434	-0.035354	3.326204
177.345938	3708.389233	6.558438	-0.035427	3.329605
177.554325	3716.448120	6.563443	-0.035471	3.333028
177.983986	3724.483687	6.568448	-0.035556	3.336446
178.338713	3732.495039	6.573453	-0.035628	3.339847
178.367988	3740.507315	6.578458	-0.035639	3.343233
178.692182	3748.555646	6.583462	-0.035704	3.346641
178.771164	3756.610429	6.588467	-0.035724	3.350040
179.011072	3764.656689	6.593472	-0.035774	3.353438
179.196660	3772.713647	6.598477	-0.035814	3.356835
179.466818	3780.665386	6.603482	-0.035870	3.360187
179.648411	3788.688523	6.608486	-0.035909	3.363562
179.775143	3796.749788	6.613491	-0.035938	3.366948
180.046683	3804.766725	6.618496	-0.035994	3.370318
180.350026	3812.814504	6.623501	-0.036056	3.373698
180.430113	3820.860192	6.628506	-0.036076	3.377065
180.683591	3828.873212	6.633510	-0.036129	3.380422
180.835887	3836.920772	6.638515	-0.036162	3.383786
180.944405	3844.942630	6.643520	-0.036188	3.387135
181.242534	3852.956655	6.648525	-0.036249	3.390484
181.397112	3861.052258	6.653530	-0.036283	3.393858
181.709396	3869.071517	6.658534	-0.036346	3.397203
181.808337	3877.041309	6.663539	-0.036370	3.400516
182.137293	3885.016468	6.668544	-0.036437	3.403836
182.318029	3893.071338	6.673549	-0.036476	3.407181
182.542535	3901.079321	6.678554	-0.036523	3.410505
182.694795	3909.148729	6.683558	-0.036556	3.413848
183.035018	3917.157069	6.688563	-0.036625	3.417169
183.117310	3925.171750	6.693568	-0.036646	3.420481
183.408463	3933.187819	6.698573	-0.036705	3.423797
183.635066	3941.199620	6.703578	-0.036753	3.427106
184.004783	3949.235742	6.708582	-0.036827	3.430427
183.979893	3957.304174	6.713587	-0.036828	3.433744
184.162233	3965.334784	6.718592	-0.036867	3.437050
184.462511	3973.356111	6.723597	-0.036928	3.440352
184.678152	3981.333443	6.728602	-0.036974	3.443631
184.560999	3989.422163	6.733606	-0.036957	3.446941
184.902621	3997.420114	6.738611	-0.037026	3.450225
185.143410	4005.476675	6.743616	-0.037077	3.453528
185.344295	4013.541948	6.748621	-0.037119	3.456829
185.485032	4021.508829	6.753626	-0.037151	3.460085
185.855791	4029.539387	6.758630	-0.037225	3.463371
186.059473	4037.572544	6.763635	-0.037268	3.466650
186.529898	4045.544809	6.768640	-0.037361	3.469909
186.893090	4053.667672	6.773645	-0.037434	3.473223
187.144820	4061.689548	6.778650	-0.037487	3.476489
187.231770	4069.679632	6.783654	-0.037508	3.479734
187.558196	4077.673956	6.788659	-0.037574	3.482985
187.660023	4085.698778	6.793664	-0.037598	3.486239
187.997223	4093.717520	6.798669	-0.037667	3.489494
188.220788	4101.762754	6.803674	-0.037714	3.492754
188.664422	4109.817960	6.808678	-0.037802	3.496021
188.723054	4117.795995	6.813683	-0.037818	3.499242
188.873197	4125.811576	6.818688	-0.037851	3.502478
189.165670	4133.850888	6.823693	-0.037911	3.505725
189.220519	4141.869378	6.828698	-0.037926	3.508953
189.586026	4149.918226	6.833702	-0.038000	3.512200
189.695314	4157.948293	6.838707	-0.038026	3.515428
189.890920	4165.934885	6.843712	-0.038067	3.518639
190.181524	4173.977003	6.848717	-0.038127	3.521872
190.127606	4181.985573	6.853722	-0.038122	3.525078
190.596187	4190.012842	6.858726	-0.038215	3.528304
190.486952	4198.066039	6.863731	-0.038200	3.531520
190.633742	4206.111284	6.868736	-0.038232	3.534738
191.095797	4214.139621	6.873741	-0.038324	3.537956
191.040535	4222.142707	6.878746	-0.038319	3.541145
191.397503	4230.157667	6.883750	-0.038391	3.544348
191.452561	4238.232231	6.888755	-0.038406	3.547563
191.586860	4246.242314	6.893760	-0.038437	3.550752
191.896623	4254.386698	6.898765	-0.038500	3.553996
192.041583	4262.382365	6.903770	-0.038532	3.557174
192.386018	4270.324955	6.908774	-0.038601	3.560333
192.704822	4278.334189	6.913779	-0.038666	3.563515
192.804041	4286.347800	6.918784	-0.038690	3.566690
192.999182	4294.366371	6.923789	-0.038732	3.569867
193.322461	4302.395542	6.928794	-0.038797	3.573048
193.726522	4310.428559	6.933798	-0.038878	3.576231
193.681518	4318.431606	6.938803	-0.038875	3.579386
193.968405	4326.435278	6.943808	-0.038933	3.582548
194.336085	4334.450680	6.948813	-0.039007	3.585714
194.340403	4342.497734	6.953818	-0.039013	3.588879
194.542161	4350.552924	6.958822	-0.039056	3.592051
194.810624	4358.566043	6.963827	-0.039112	3.595205
194.886906	4366.576070	6.968832	-0.039131	3.598349
195.258175	4374.599380	6.973837	-0.039206	3.601504
195.564592	4382.550730	6.978842	-0.039268	3.604627
195.836675	4390.611319	6.983846	-0.039324	3.607788
195.988157	4398.659601	6.988851	-0.039357	3.610938
196.338322	4406.686701	6.993856	-0.039428	3.614083
196.633553	4414.727992	6.998861	-0.039488	3.617229
196.694002	4422.729464	7.003866	-0.039505	3.620350
197.057682	4430.746517	7.008870	-0.039578	3.623483
197.334898	4438.799931	7.013875	-0.039635	3.626625
197.352264	4446.812516	7.018880	-0.039644	3.629742
197.830533	4454.890352	7.023885	-0.039738	3.632893
198.189781	4462.904736	7.028890	-0.039810	3.636014
198.331001	4470.898399	7.033894	-0.039842	3.639118
198.430549	4478.926782	7.038899	-0.039866	3.642232
198.564102	4486.906538	7.043904	-0.039896	3.645325
198.919133	4494.950793	7.048909	-0.039967	3.648447
198.977275	4502.993882	7.053914	-0.039983	3.651557
199.302056	4511.035605	7.058918	-0.040049	3.654671
199.512178	4519.081520	7.063923	-0.040094	3.657781
199.628130	4527.067781	7.068928	-0.040121	3.660863
199.895611	4535.106659	7.073933	-0.040176	3.663967
200.074023	4543.121893	7.078938	-0.040214	3.667057
200.231052	4551.160826	7.083942	-0.040249	3.670152
200.645980	4559.180611	7.088947	-0.040332	3.673244
200.953492	4567.193284	7.093952	-0.040394	3.676328
201.424772	4575.183328	7.098957	-0.040487	3.679405
201.224109	4583.201537	7.103962	-0.040455	3.682473
201.604490	4591.222605	7.108966	-0.040531	3.685554
201.867625	4599.253311	7.113971	-0.040586	3.688633
201.830375	4607.301392	7.118976	-0.040584	3.691709
202.001343	4615.354947	7.123981	-0.040621	3.694789
202.319265	4623.342797	7.128986	-0.040686	3.697846
202.500940	4631.365020	7.133990	-0.040725	3.700909
202.778114	4639.359155	7.138995	-0.040782	3.703962
202.813610	4647.401743	7.144000	-0.040794	3.707025
203.100545	4655.436598	7.149005	-0.040853	3.710088
203.169285	4663.509371	7.154010	-0.040871	3.713158
203.561273	4671.574938	7.159014	-0.040949	3.716230
203.882569	4679.511898	7.164019	-0.041014	3.719250
203.753898	4687.538195	7.169024	-0.040996	3.722290
204.037686	4695.525295	7.174029	-0.041054	3.725322
204.232045	4703.523812	7.179034	-0.041095	3.728354
204.548021	4711.592362	7.184038	-0.041160	3.731413
204.528364	4719.636506	7.189043	-0.041161	3.734452
204.659062	4727.657190	7.194048	-0.041191	3.737484
205.090152	4735.662557	7.199053	-0.041277	3.740514
204.977187	4743.699878	7.204058	-0.041261	3.743541
205.324783	4751.708717	7.209062	-0.041331	3.746566
205.460892	4759.710592	7.214067	-0.041362	3.749580
205.699974	4767.760857	7.219072	-0.041411	3.752613
205.950774	4775.820360	7.224077	-0.041463	3.755647
206.127419	4783.790335	7.229082	-0.041502	3.758643
206.346368	4791.836632	7.234086	-0.041548	3.761666
206.313360	4799.810539	7.239091	-0.041547	3.764654
206.658593	4807.839760	7.244096	-0.041617	3.767669
207.074053	4815.890562	7.249101	-0.041699	3.770691
207.163198	4823.897332	7.254106	-0.041721	3.773687
207.462259	4831.963224	7.259110	-0.041782	3.776708
207.560981	4839.958076	7.264115	-0.041806	3.779694
207.789196	4848.006909	7.269120	-0.041854	3.782702
207.783515	4856.024920	7.274125	-0.041858	3.785690
207.926346	4863.996105	7.279130	-0.041890	3.788662
208.306880	4872.078045	7.284134	-0.041966	3.791678
208.282726	4880.104524	7.289139	-0.041967	3.794662
208.633155	4888.116383	7.294144	-0.042038	3.797646
208.699619	4896.113300	7.299149	-0.042055	3.800617
208.877009	4904.102526	7.304154	-0.042094	3.803584
209.162508	4912.124717	7.309158	-0.042152	3.806564
209.384287	4920.140959	7.314163	-0.042199	3.809537
209.559768	4928.181405	7.319168	-0.042237	3.812517
209.695848	4936.236381	7.324173	-0.042268	3.815498
209.970072	4944.231561	7.329178	-0.042324	3.818458
210.240161	4952.247687	7.334182	-0.042380	3.821423
210.606843	4960.234243	7.339187	-0.042453	3.824377
210.788765	4968.268019	7.344192	-0.042492	3.827343
211.130137	4976.300037	7.349197	-0.042561	3.830308
211.267150	4984.343045	7.354202	-0.042592	3.833271
211.360928	4992.365873	7.359206	-0.042615	3.836224
211.420071	5000.403646	7.364211	-0.042631	3.839179
211.509849	5008.431496	7.369216	-0.042653	3.842129
211.720082	5016.393396	7.374221	-0.042698	3.845054
211.730115	5024.427798	7.379226	-0.042705	3.848000
212.269352	5032.440329	7.384230	-0.042811	3.850946
212.459660	5040.533676	7.389235	-0.042852	3.853913
212.426003	5048.543029	7.394240	-0.042851	3.856842
213.008281	5056.519218	7.399245	-0.042964	3.859769
213.190774	5064.524944	7.404250	-0.043004	3.862696
213.580407	5072.533426	7.409254	-0.043082	3.865627
213.807495	5080.634781	7.414259	-0.043129	3.868585
214.057087	5088.623824	7.419264	-0.043181	3.871501
214.186450	5096.921311	7.424269	-0.043211	3.874525
214.214674	5104.840954	7.429274	-0.043221	3.877407
214.687720	5112.730214	7.434278	-0.043315	3.880284
214.794618	5120.747043	7.439283	-0.043340	3.883198
214.702225	5128.733898	7.444288	-0.043328	3.886096
215.159873	5136.771244	7.449293	-0.043418	3.889020
215.255101	5144.783657	7.454298	-0.043441	3.891926
215.424366	5152.811218	7.459302	-0.043478	3.894837
215.897585	5160.808515	7.464307	-0.043572	3.897740
216.111178	5168.813202	7.469312	-0.043617	3.900639
216.051624	5176.841345	7.474317	-0.043611	3.903539
216.186578	5184.866413	7.479322	-0.043642	3.906439
216.358269	5192.904305	7.484326	-0.043679	3.909342
216.744043	5200.937450	7.489331	-0.043756	3.912246
216.803307	5208.955876	7.494336	-0.043772	3.915136
217.212695	5216.986150	7.499341	-0.043854	3.918034
217.184821	5224.945395	7.504346	-0.043854	3.920897
217.399546	5232.963558	7.509350	-0.043899	3.923784
217.633243	5240.995480	7.514355	-0.043948	3.926673
217.815035	5248.999442	7.519360	-0.043988	3.929549
218.102616	5257.070334	7.524365	-0.044046	3.932449
217.985442	5265.056444	7.529370	-0.044030	3.935310
218.419879	5273.071161	7.534374	-0.044116	3.938188
218.630414	5281.088834	7.539379	-0.044161	3.941061
218.597475	5289.095398	7.544384	-0.044160	3.943924
218.842682	5297.154691	7.549389	-0.044211	3.946808
218.982899	5305.150686	7.554394	-0.044242	3.949666
219.340711	5313.193794	7.559398	-0.044314	3.952543
219.436491	5321.258000	7.564403	-0.044338	3.955420
219.641087	5329.236206	7.569408	-0.044381	3.958266
219.968937	5337.246894	7.574413	-0.044447	3.961124
220.002480	5345.233439	7.579418	-0.044459	3.963966
220.389417	5353.233816	7.584422	-0.044536	3.966817
220.589768	5361.264628	7.589427	-0.044579	3.969674
220.557005	5369.310361	7.594432	-0.044578	3.972530
220.781639	5377.342077	7.599437	-0.044625	3.975383
221.217439	5385.333846	7.604442	-0.044712	3.978224
221.407067	5393.359532	7.609446	-0.044752	3.981070
221.546078	5401.370419	7.614451	-0.044784	3.983908
221.644414	5409.393344	7.619456	-0.044807	3.986748
222.192454	5417.458272	7.624461	-0.044915	3.989608
222.195856	5425.448508	7.629466	-0.044921	3.992430
222.384114	5433.536107	7.634470	-0.044961	3.995288
222.724882	5441.553729	7.639475	-0.045030	3.998122
222.702221	5449.542814	7.644480	-0.045031	4.000937
223.022877	5457.572897	7.649485	-0.045096	4.003771
223.090444	5465.591550	7.654490	-0.045114	4.006594
223.462573	5473.593682	7.659494	-0.045189	4.009415
223.582138	5481.636613	7.664499	-0.045216	4.012244
223.526693	5489.651082	7.669504	-0.045211	4.015058
224.227952	5497.682961	7.674509	-0.045347	4.017888
224.173017	5505.708801	7.679514	-0.045342	4.020702
224.316292	5513.691668	7.684518	-0.045374	4.023502
224.428876	5521.730513	7.689523	-0.045401	4.026319
224.578611	5529.753838	7.694528	-0.045434	4.029130
224.904797	5537.783424	7.699533	-0.045500	4.031943
225.001179	5545.885606	7.704538	-0.045523	4.034776
225.241389	5553.860543	7.709542	-0.045573	4.037565
225.383868	5561.838905	7.714547	-0.045605	4.040352
225.678328	5569.770880	7.719552	-0.045665	4.043122
225.935379	5577.844378	7.724557	-0.045718	4.045940
226.020366	5585.856256	7.729562	-0.045740	4.048732
226.273865	5593.882080	7.734566	-0.045792	4.051529
226.626815	5601.899645	7.739571	-0.045863	4.054322
226.745782	5609.926069	7.744576	-0.045891	4.057114
226.754019	5617.927467	7.749581	-0.045897	4.059893
227.094836	5625.930937	7.754586	-0.045966	4.062676
227.442583	5633.937967	7.759590	-0.046036	4.065458
227.791840	5642.007343	7.764595	-0.046107	4.068259
227.510222	5649.970276	7.769600	-0.046060	4.071013
227.957105	5658.044327	7.774605	-0.046148	4.073814
228.260814	5666.035821	7.779610	-0.046210	4.076583
228.463990	5674.053053	7.784614	-0.046253	4.079356
228.648834	5682.105477	7.789619	-0.046293	4.082140
228.779775	5690.034365	7.794624	-0.046323	4.084879
229.084602	5698.125854	7.799629	-0.046385	4.087674
228.798072	5706.152220	7.804634	-0.046337	4.090437
229.208371	5714.199203	7.809638	-0.046419	4.093214
229.503908	5722.168155	7.814643	-0.046479	4.095961
229.777123	5730.167028	7.819648	-0.046535	4.098717
230.209307	5738.196364	7.824653	-0.046621	4.101482
230.630859	5746.149885	7.829658	-0.046705	4.104220
230.777051	5754.220039	7.834662	-0.046737	4.106992
231.126182	5762.258225	7.839667	-0.046808	4.109754
231.415803	5770.300502	7.844672	-0.046867	4.112515
231.424162	5778.363994	7.849677	-0.046874	4.115278
231.542111	5786.389733	7.854682	-0.046901	4.118027
231.794602	5794.343950	7.859686	-0.046953	4.120752
231.953551	5802.377217	7.864691	-0.046988	4.123500
232.084797	5810.361146	7.869696	-0.047018	4.126230
232.186824	5818.399932	7.874701	-0.047042	4.128976
232.277456	5826.438114	7.879706	-0.047065	4.131720
232.619475	5834.502210	7.884710	-0.047134	4.134474
232.724151	5842.525090	7.889715	-0.047159	4.137209
232.988361	5850.484540	7.894720	-0.047213	4.139923
233.269604	5858.555198	7.899725	-0.047271	4.142673
233.182839	5866.528203	7.904730	-0.047260	4.145383
233.579072	5874.559836	7.909734	-0.047339	4.148117
233.824702	5882.588232	7.914739	-0.047390	4.150847
233.843451	5890.625035	7.919744	-0.047399	4.153575
234.040010	5898.668572	7.924749	-0.047441	4.156305
234.137736	5906.603754	7.929754	-0.047464	4.158996
234.306083	5914.676399	7.934758	-0.047501	4.161733
234.565447	5922.673033	7.939763	-0.047555	4.164443
234.691706	5930.674713	7.944768	-0.047584	4.167151
235.030693	5938.721881	7.949773	-0.047652	4.169875
235.027197	5946.766996	7.954778	-0.047657	4.172593
235.295018	5954.780009	7.959782	-0.047712	4.175301
235.431394	5962.840471	7.964787	-0.047743	4.178023
235.489583	5970.761458	7.969792	-0.047759	4.180694
235.700194	5978.780070	7.974797	-0.047803	4.183398
236.055521	5986.769772	7.979802	-0.047875	4.186093
236.262075	5994.794445	7.984806	-0.047919	4.188795
236.515942	6002.842437	7.989811	-0.047971	4.191505
236.497604	6010.981207	7.994816	-0.047973	4.194240
236.713745	6019.014019	7.999821	-0.048019	4.196940
236.803110	6026.927533	8.004826	-0.048041	4.199597
237.164112	6034.897532	8.009830	-0.048113	4.202274
237.453531	6042.877700	8.014835	-0.048173	4.204952
237.540621	6050.910094	8.019840	-0.048194	4.207644
237.757037	6058.931742	8.024845	-0.048240	4.210332
237.907526	6066.979209	8.029850	-0.048273	4.213026
237.915719	6075.000537	8.034854	-0.048280	4.215708
238.250266	6083.036262	8.039859	-0.048348	4.218396
238.654473	6091.020086	8.044864	-0.048428	4.221066
238.841712	6099.032156	8.049869	-0.048468	4.223742
238.924941	6107.052330	8.054874	-0.048489	4.226417
239.285492	6115.046421	8.059878	-0.048562	4.229085
239.482619	6123.107463	8.064883	-0.048604	4.231772
239.599622	6131.118703	8.069888	-0.048631	4.234440
239.892480	6139.209081	8.074893	-0.048691	4.237134
239.738677	6147.106489	8.079898	-0.048667	4.239758
240.025139	6155.175412	8.084902	-0.048726	4.242441
240.383120	6163.155469	8.089907	-0.048798	4.245094
240.577071	6171.173284	8.094912	-0.048839	4.247756
240.872270	6179.201068	8.099917	-0.048900	4.250421
240.979195	6187.239911	8.104922	-0.048925	4.253086
241.297201	6195.308516	8.109926	-0.048990	4.255761
241.353822	6203.340982	8.114931	-0.049006	4.258420
241.414688	6211.313242	8.119936	-0.049022	4.261057
241.827552	6219.308895	8.124941	-0.049104	4.263704
241.872910	6227.318047	8.129946	-0.049118	4.266350
242.185843	6235.368992	8.134950	-0.049182	4.269010
242.245997	6243.447485	8.139955	-0.049198	4.271676
242.469251	6251.454097	8.144960	-0.049245	4.274318
242.558816	6259.512634	8.149965	-0.049267	4.276974
242.583030	6267.440309	8.154970	-0.049277	4.279585
242.896273	6275.455065	8.159974	-0.049341	4.282225
243.242040	6283.443741	8.164979	-0.049410	4.284856
243.251158	6291.485368	8.169984	-0.049417	4.287499
243.665426	6299.513877	8.174989	-0.049500	4.290140
243.889973	6307.570012	8.179994	-0.049547	4.292786
244.052685	6315.553645	8.184998	-0.049583	4.295407
244.068609	6323.626553	8.190003	-0.049591	4.298054
244.029876	6331.537010	8.195008	-0.049589	4.300646
244.405487	6339.606905	8.200013	-0.049664	4.303291
244.542615	6347.594702	8.205018	-0.049695	4.305907
244.910504	6355.625270	8.210022	-0.049769	4.308536
245.067127	6363.656943	8.215027	-0.049804	4.311163
244.893648	6371.696947	8.220032	-0.049777	4.313788
245.122100	6379.730247	8.225037	-0.049825	4.316412
245.489963	6387.693772	8.230042	-0.049898	4.319013
245.616658	6395.698008	8.235046	-0.049927	4.321624
245.634560	6403.744883	8.240051	-0.049936	4.324247
245.760366	6411.718664	8.245056	-0.049965	4.326844
246.038416	6419.758445	8.250061	-0.050022	4.329463
246.333876	6427.816300	8.255066	-0.050082	4.332086
246.469379	6435.818996	8.260070	-0.050113	4.334689
246.510972	6443.856316	8.265075	-0.050126	4.337300
246.699789	6451.813838	8.270080	-0.050166	4.339885
246.895702	6459.892496	8.275085	-0.050208	4.342508
247.206003	6467.849683	8.280090	-0.050271	4.345091
247.378954	6475.856772	8.285094	-0.050309	4.347687
247.549495	6483.931439	8.290099	-0.050346	4.350303
247.614975	6491.955139	8.295104	-0.050363	4.352901
248.012289	6500.089462	8.300109	-0.050443	4.355535
247.888107	6508.026958	8.305114	-0.050425	4.358101
248.125974	6515.952825	8.310118	-0.050475	4.360664
248.258931	6523.986886	8.315123	-0.050505	4.363259
248.553806	6531.950334	8.320128	-0.050565	4.365831
248.796236	6539.979556	8.325133	-0.050615	4.368422
249.079469	6547.990658	8.330138	-0.050673	4.371006
249.290924	6556.022402	8.335142	-0.050718	4.373595
249.486264	6564.130076	8.340147	-0.050760	4.376206
249.654469	6572.085916	8.345152	-0.050797	4.378767
250.171076	6580.074673	8.350157	-0.050898	4.381339
250.064836	6588.133006	8.355162	-0.050884	4.383929
250.184439	6596.135033	8.360166	-0.050911	4.386500
250.553960	6604.178653	8.365171	-0.050985	4.389084
250.558000	6612.181380	8.370176	-0.050991	4.391651
250.593586	6620.228239	8.375181	-0.051003	4.394232
250.856432	6628.248071	8.380186	-0.051058	4.396803
251.213486	6636.193262	8.385190	-0.051129	4.399349
251.305001	6644.248684	8.390195	-0.051152	4.401928
251.518605	6652.183071	8.395200	-0.051197	4.404467
251.788380	6660.281505	8.400205	-0.051253	4.407057
251.757692	6668.288502	8.405210	-0.051252	4.409616
252.107169	6676.332850	8.410214	-0.051323	4.412186
252.295572	6684.326574	8.415219	-0.051363	4.414738
252.364145	6692.387379	8.420224	-0.051381	4.417309
252.491112	6700.373739	8.425229	-0.051410	4.419855
252.538394	6708.424657	8.430234	-0.051424	4.422421
252.769380	6716.377783	8.435238	-0.051473	4.424954
253.015314	6724.454122	8.440243	-0.051524	4.427525
253.043668	6732.388811	8.445248	-0.051534	4.430048
253.426564	6740.503339	8.450253	-0.051611	4.432629
253.500389	6748.538148	8.455258	-0.051630	4.435181
253.552698	6756.537557	8.460262	-0.051645	4.437721
253.622529	6764.493136	8.465267	-0.051663	4.440246
253.769875	6772.533108	8.470272	-0.051696	4.442796
254.131515	6780.523023	8.475277	-0.051769	4.445329
254.269513	6788.576431	8.480282	-0.051800	4.447880
254.481202	6796.548848	8.485286	-0.051845	4.450405
254.648083	6804.658656	8.490291	-0.051881	4.452971
254.806181	6812.605408	8.495296	-0.051916	4.455484
254.834147	6820.673742	8.500301	-0.051926	4.458034
255.113836	6828.649129	8.505306	-0.051984	4.460554
255.128762	6836.670476	8.510310	-0.051992	4.463086
255.532852	6844.672634	8.515315	-0.052072	4.465612
255.658026	6852.647607	8.520320	-0.052101	4.468126
255.875924	6860.702535	8.525325	-0.052147	4.470665
256.035419	6868.781538	8.530330	-0.052182	4.473210
256.302849	6876.749105	8.535334	-0.052237	4.475718
256.438642	6884.788980	8.540339	-0.052268	4.478248
256.555549	6892.730327	8.545344	-0.052295	4.480745
256.925513	6900.812082	8.550349	-0.052369	4.483285
256.951737	6908.794131	8.555354	-0.052379	4.485792
256.917787	6916.819975	8.560359	-0.052378	4.488311
257.372776	6924.823410	8.565363	-0.052468	4.490822
257.606390	6932.834284	8.570368	-0.052517	4.493334
257.873882	6940.896322	8.575373	-0.052572	4.495861
258.001146	6948.910226	8.580378	-0.052601	4.498371
258.268358	6956.917646	8.585383	-0.052657	4.500877
258.568832	6964.920419	8.590387	-0.052718	4.503381
258.587084	6972.889797	8.595392	-0.052726	4.505873
258.871478	6980.965733	8.600397	-0.052785	4.508396
259.060181	6988.970944	8.605402	-0.052825	4.510897
259.111065	6997.055613	8.610407	-0.052840	4.513420
259.295580	7005.089936	8.615411	-0.052880	4.515926
259.422966	7013.023964	8.620416	-0.052909	4.518400
259.466072	7021.018017	8.625421	-0.052922	4.520890
259.639569	7029.018775	8.630426	-0.052960	4.523382
259.661640	7037.004779	8.635431	-0.052969	4.525867
259.720529	7045.070294	8.640435	-0.052986	4.528376
259.816694	7053.039671	8.645440	-0.053009	4.530854
260.069306	7061.124261	8.650445	-0.053061	4.533366
260.277309	7069.086938	8.655450	-0.053105	4.535839
260.482743	7077.102360	8.660455	-0.053149	4.538327
260.810328	7085.128795	8.665459	-0.053215	4.540817
260.865352	7093.108504	8.670464	-0.053231	4.543291
260.973248	7101.161931	8.675469	-0.053256	4.545786
261.288406	7109.205960	8.680474	-0.053320	4.548278
261.566305	7117.199167	8.685479	-0.053377	4.550752
261.725538	7125.255787	8.690483	-0.053412	4.553244
261.718291	7133.287105	8.695488	-0.053416	4.555727
261.956271	7141.270553	8.700493	-0.053466	4.558194
262.095417	7149.213190	8.705498	-0.053497	4.560647
262.151590	7157.268634	8.710503	-0.053513	4.563134
262.340403	7165.309973	8.715507	-0.053553	4.565614
262.381517	7173.289230	8.720512	-0.053566	4.568074
262.629157	7181.327142	8.725517	-0.053618	4.570551
262.759001	7189.374793	8.730522	-0.053647	4.573030
262.954761	7197.369954	8.735527	-0.053689	4.575491
263.276863	7205.443439	8.740531	-0.053754	4.577975
263.208502	7213.375632	8.745536	-0.053747	4.580414
263.527818	7221.474263	8.750541	-0.053812	4.582903
263.829001	7229.423913	8.755546	-0.053873	4.585344
263.772450	7237.440176	8.760551	-0.053868	4.587805
264.014261	7245.489126	8.765555	-0.053918	4.590275
264.270683	7253.495664	8.770560	-0.053972	4.592730
264.635808	7261.574872	8.775565	-0.054045	4.595206
264.787849	7269.598385	8.780570	-0.054079	4.597664
264.890526	7277.555853	8.785575	-0.054103	4.600100
265.039300	7285.614574	8.790579	-0.054136	4.602565
265.031131	7293.482512	8.795584	-0.054140	4.604972
265.070979	7301.569174	8.800589	-0.054153	4.607443
265.491912	7309.587068	8.805594	-0.054236	4.609892
265.582772	7317.620180	8.810599	-0.054259	4.612345
265.809989	7325.677277	8.815603	-0.054306	4.614804
265.929145	7333.664850	8.820608	-0.054334	4.617240
265.929626	7341.651335	8.825613	-0.054339	4.619674
266.254995	7349.697084	8.830618	-0.054405	4.622125
266.497773	7357.649614	8.835623	-0.054456	4.624547
266.835805	7365.745185	8.840627	-0.054524	4.627010
266.631146	7373.711255	8.845632	-0.054491	4.629434
266.962934	7381.756991	8.850637	-0.054558	4.631879
267.143670	7389.800469	8.855642	-0.054597	4.634323
267.237358	7397.796563	8.860647	-0.054620	4.636752
267.362148	7405.783630	8.865651	-0.054648	4.639176
267.575476	7413.796883	8.870656	-0.054694	4.641607
267.977766	7421.812091	8.875661	-0.054774	4.644037
267.920701	7429.780282	8.880666	-0.054768	4.646451
268.204871	7437.830388	8.885671	-0.054827	4.648889
268.424038	7445.896922	8.890675	-0.054873	4.651331
268.393647	7453.878872	8.895680	-0.054873	4.653746
268.541703	7461.932970	8.900685	-0.054905	4.656182
268.883574	7469.927262	8.905690	-0.054974	4.658598
269.044629	7477.935213	8.910695	-0.055010	4.661016
269.296446	7485.969618	8.915699	-0.055062	4.663442
269.271696	7493.934287	8.920704	-0.055063	4.665846
269.523900	7502.008241	8.925709	-0.055115	4.668280
269.593719	7510.027388	8.930714	-0.055133	4.670698
269.760526	7518.053412	8.935719	-0.055170	4.673116
270.228419	7526.142668	8.940723	-0.055262	4.675551
270.197804	7534.143749	8.945728	-0.055262	4.677959
270.368254	7542.042387	8.950733	-0.055299	4.680335
270.560951	7550.104172	8.955738	-0.055340	4.682759
270.593321	7558.014214	8.960743	-0.055351	4.685136
270.651608	7566.102110	8.965747	-0.055368	4.687565
270.970634	7574.058938	8.970752	-0.055432	4.689953
271.302418	7582.135576	8.975757	-0.055500	4.692376
271.507583	7590.145734	8.980762	-0.055543	4.694777
271.397531	7598.110582	8.985767	-0.055528	4.697165
271.791170	7606.179625	8.990771	-0.055607	4.699582
272.031245	7614.200545	8.995776	-0.055657	4.701983
272.199773	7622.191641	9.000781	-0.055693	4.704374
272.386267	7630.251766	9.005786	-0.055733	4.706784
272.505610	7638.193271	9.010791	-0.055761	4.709158
272.664919	7646.251037	9.015795	-0.055796	4.711566
272.617075	7654.249299	9.020800	-0.055792	4.713955
272.873787	7662.322614	9.025805	-0.055845	4.716364
272.936792	7670.312388	9.030810	-0.055863	4.718748
273.106502	7678.272773	9.035815	-0.055899	4.721121
273.353795	7686.312437	9.040819	-0.055951	4.723516
273.537020	7694.295853	9.045824	-0.055990	4.725894
273.595041	7702.377449	9.050829	-0.056006	4.728300
273.819190	7710.397872	9.055834	-0.056054	4.730686
273.917667	7718.425224	9.060839	-0.056077	4.733074
274.090937	7726.431273	9.065843	-0.056115	4.735453
274.229999	7734.465197	9.070848	-0.056146	4.737840
274.480070	7742.451975	9.075853	-0.056198	4.740211
274.672648	7750.517909	9.080858	-0.056239	4.742605
274.688793	7758.400597	9.085863	-0.056247	4.744944
274.937948	7766.499642	9.090867	-0.056299	4.747345
275.293039	7774.496763	9.095872	-0.056371	4.749713
275.309551	7782.573793	9.100877	-0.056379	4.752106
275.426801	7790.604542	9.105882	-0.056406	4.754484
275.536285	7798.541129	9.110887	-0.056432	4.756832
275.836377	7806.592983	9.115891	-0.056493	4.759213
275.862936	7814.561827	9.120896	-0.056503	4.761568
276.076958	7822.556245	9.125901	-0.056549	4.763930
276.231979	7830.573983	9.130906	-0.056583	4.766297
276.191788	7838.601466	9.135911	-0.056581	4.768667
276.497433	7846.661199	9.140915	-0.056643	4.771044
276.738744	7854.651074	9.145920	-0.056693	4.773399
276.838257	7862.711761	9.150925	-0.056717	4.775775
277.002547	7870.701163	9.155930	-0.056753	4.778128
277.221315	7878.679494	9.160935	-0.056799	4.780476
277.254945	7886.708861	9.165939	-0.056811	4.782839
277.261950	7894.672805	9.170944	-0.056817	4.785182
277.582269	7902.739065	9.175949	-0.056882	4.787552
277.751058	7910.760281	9.180954	-0.056919	4.789909
277.724263	7918.792990	9.185959	-0.056919	4.792268
277.992455	7926.782364	9.190963	-0.056975	4.794613
277.996806	7934.838433	9.195968	-0.056981	4.796977
278.206389	7942.776290	9.200973	-0.057025	4.799304
278.495326	7950.849390	9.205978	-0.057084	4.801669
278.465165	7958.735678	9.210983	-0.057084	4.803980
278.748314	7966.875370	9.215987	-0.057142	4.806362
278.850668	7974.865626	9.220992	-0.057166	4.808701
279.150019	7982.949768	9.225997	-0.057227	4.811064
279.311613	7990.354249	9.231002	-0.057263	4.813229
279.333037	7994.887146	9.236007	-0.057270	4.814554

279.593790	7997.247262	9.241011	-0.057320	4.815242
279.736594	7998.628008	9.246016	-0.057347	4.815645
279.849573	7999.263630	9.251021	-0.057369	4.815830
279.646840	7999.867904	9.256026	-0.057332	4.816008
279.707052	7999.800627	9.261031	-0.057343	4.815988
279.825074	7999.916037	9.266035	-0.057365	4.816021
279.725266	7999.819143	9.271040	-0.057347	4.815993
279.954013	7999.811554	9.276045	-0.057389	4.815990
280.058539	7999.927788	9.281050	-0.057409	4.816023
279.960961	7999.874741	9.286055	-0.057391	4.816008
280.164425	7999.882720	9.291059	-0.057429	4.816009
280.193725	7999.814881	9.296064	-0.057434	4.815989
280.307383	7999.837257	9.301069	-0.057456	4.815995
280.328450	7999.883594	9.306074	-0.057460	4.816009
280.474019	7999.793291	9.311079	-0.057487	4.815981
280.375862	7999.905847	9.316083	-0.057469	4.816015
280.424735	7999.897129	9.321088	-0.057478	4.816012
280.456846	7999.901997	9.326093	-0.057484	4.816013
280.539786	7999.928089	9.331098	-0.057500	4.816020
280.516061	7999.875313	9.336103	-0.057495	4.816005
280.669328	7999.958244	9.341107	-0.057524	4.816029
280.692663	7999.970432	9.346112	-0.057528	4.816032
280.828049	7999.915204	9.351117	-0.057554	4.816015
280.626763	7999.963914	9.356122	-0.057516	4.816030
280.934118	7999.885098	9.361127	-0.057574	4.816006
280.996471	7999.939666	9.366131	-0.057585	4.816021
280.844038	7999.893099	9.371136	-0.057557	4.816009
280.924838	7999.969372	9.376141	-0.057572	4.816030
280.867947	7999.953391	9.381146	-0.057562	4.816026
280.830383	7999.932418	9.386151	-0.057555	4.816020
280.782609	7999.961478	9.391155	-0.057546	4.816029
281.069415	7999.960289	9.396160	-0.057600	4.816027
281.107963	7999.922534	9.401165	-0.057607	4.816016
281.271567	7999.949024	9.406170	-0.057638	4.816023
281.198674	7999.976560	9.411175	-0.057624	4.816031
281.180768	7999.960218	9.416179	-0.057621	4.816026
281.258065	7999.944537	9.421184	-0.057635	4.816021
281.239987	7999.954905	9.426189	-0.057632	4.816025
281.442601	7999.981036	9.431194	-0.057670	4.816031
281.388618	7999.927709	9.436199	-0.057660	4.816016
281.603836	7999.982919	9.441203	-0.057700	4.816031
281.475193	7999.928235	9.446208	-0.057676	4.816015
281.524362	7999.992181	9.451213	-0.057686	4.816034
281.186996	7999.952938	9.456218	-0.057623	4.816024
281.266586	7999.903107	9.461223	-0.057638	4.816009
281.407848	7999.987959	9.466227	-0.057664	4.816033
281.323683	7999.972550	9.471232	-0.057649	4.816029
281.298045	7999.912259	9.476237	-0.057644	4.816012
281.296082	7999.929330	9.481242	-0.057644	4.816017
281.433676	7999.916882	9.486247	-0.057670	4.816012
281.613656	7999.950081	9.491251	-0.057703	4.816021
281.400237	7999.909885	9.496256	-0.057664	4.816010
281.591796	7999.935815	9.501261	-0.057699	4.816017
281.845639	7999.988522	9.506266	-0.057747	4.816031
281.828272	7999.982874	9.511271	-0.057744	4.816030
281.784993	7999.992784	9.516275	-0.057736	4.816033
281.769347	7999.966866	9.521280	-0.057733	4.816025
281.826469	7999.921968	9.526285	-0.057744	4.816012
281.794952	7999.939571	9.531290	-0.057738	4.816017
281.774595	7999.897540	9.536295	-0.057734	4.816005
281.725608	7999.973594	9.541299	-0.057725	4.816027
281.741290	7999.941834	9.546304	-0.057728	4.816018
281.980449	7999.953671	9.551309	-0.057773	4.816020
281.767187	7999.988272	9.556314	-0.057733	4.816031
281.873303	7999.874812	9.561319	-0.057753	4.815998
282.038411	7999.957962	9.566323	-0.057784	4.816021
281.970174	7999.897964	9.571328	-0.057771	4.816004
281.745999	7999.929162	9.576333	-0.057730	4.816014
281.860260	7999.973990	9.581338	-0.057751	4.816027
282.087771	7999.907613	9.586343	-0.057794	4.816006
282.088922	7999.993127	9.591347	-0.057794	4.816031
281.704304	7999.928448	9.596352	-0.057722	4.816014
281.834368	7999.919068	9.601357	-0.057747	4.816011
281.920276	8000.017876	9.606362	-0.057763	4.816039
281.878939	7999.981874	9.611367	-0.057755	4.816029
282.084435	8000.015539	9.616371	-0.057794	4.816038
282.215382	7999.926036	9.621376	-0.057818	4.816011
281.995118	7999.917769	9.626381	-0.057777	4.816010
282.172467	7999.961608	9.631386	-0.057810	4.816021
282.205951	7999.955816	9.636391	-0.057817	4.816020
282.120791	7999.985266	9.641395	-0.057801	4.816029
281.893956	7999.960852	9.646400	-0.057759	4.816023
281.999073	7999.930718	9.651405	-0.057778	4.816013
281.998068	7999.958492	9.656410	-0.057778	4.816021
281.864429	7999.976376	9.661415	-0.057754	4.816027
282.272238	7999.999827	9.666419	-0.057830	4.816032
282.275648	7999.971049	9.671424	-0.057830	4.816024
282.279063	8000.001041	9.676429	-0.057831	4.816032
282.400505	8000.000054	9.681434	-0.057854	4.816031
282.228315	7999.946713	9.686439	-0.057822	4.816017
282.214320	8000.010582	9.691443	-0.057819	4.816035
282.093099	7999.998772	9.696448	-0.057797	4.816033
282.143487	8000.021070	9.701453	-0.057807	4.816039
282.310904	8000.005959	9.706458	-0.057838	4.816034
282.230613	7999.916890	9.711463	-0.057823	4.816008
282.249745	8000.007005	9.716467	-0.057827	4.816034
282.309718	7999.955748	9.721472	-0.057838	4.816019
282.272131	7999.933705	9.726477	-0.057831	4.816013
282.430989	7999.953700	9.731482	-0.057861	4.816018
282.462195	7999.917948	9.736487	-0.057867	4.816007
282.457417	7999.953134	9.741491	-0.057866	4.816017
282.564226	7999.963634	9.746496	-0.057886	4.816020
282.715910	7999.930072	9.751501	-0.057914	4.816009
282.609744	7999.995471	9.756506	-0.057895	4.816029
282.450836	7999.890014	9.761511	-0.057865	4.815999
282.490398	7999.951650	9.766515	-0.057872	4.816017
282.622708	7999.944449	9.771520	-0.057897	4.816014
282.652214	7999.937517	9.776525	-0.057903	4.816012
282.534514	7999.989883	9.781530	-0.057881	4.816028
282.370401	7999.912113	9.786535	-0.057851	4.816006
282.549973	7999.934622	9.791539	-0.057884	4.816011
282.498618	7999.954001	9.796544	-0.057875	4.816017
282.547970	7999.935676	9.801549	-0.057884	4.816012
282.618122	7999.977566	9.806554	-0.057897	4.816024
282.633800	7999.887036	9.811559	-0.057900	4.815997
282.720180	7999.926016	9.816563	-0.057916	4.816008
282.587925	7999.915074	9.821568	-0.057892	4.816005
282.676984	7999.944486	9.826573	-0.057909	4.816014
282.823253	7999.998446	9.831578	-0.057936	4.816029
282.720649	7999.861955	9.836583	-0.057917	4.815989
282.653487	7999.944091	9.841587	-0.057905	4.816014
282.631677	7999.912718	9.846592	-0.057901	4.816005
282.730294	7999.935892	9.851597	-0.057919	4.816011
282.783580	7999.961448	9.856602	-0.057929	4.816018
282.542665	7999.939983	9.861607	-0.057884	4.816013
282.630284	7999.969368	9.866611	-0.057901	4.816021
282.626969	7999.968250	9.871616	-0.057900	4.816021
282.841229	7999.967882	9.876621	-0.057940	4.816020
282.644172	7999.998504	9.881626	-0.057904	4.816030
282.627939	7999.983260	9.886631	-0.057901	4.816025
283.073793	7999.893070	9.891635	-0.057984	4.815996
282.880403	7999.938718	9.896640	-0.057948	4.816011
282.723598	7999.891000	9.901645	-0.057919	4.815998
282.906400	7999.941350	9.906650	-0.057953	4.816011
282.881530	7999.976170	9.911655	-0.057949	4.816022
282.929082	8000.000554	9.916659	-0.057958	4.816029
282.863625	7999.917096	9.921664	-0.057945	4.816005
282.910893	7999.925446	9.926669	-0.057954	4.816007
282.797313	7999.975751	9.931674	-0.057933	4.816022
282.847511	7999.955303	9.936679	-0.057943	4.816016
282.778118	7999.978629	9.941683	-0.057930	4.816023
282.642638	7999.953737	9.946688	-0.057905	4.816016
282.895392	7999.913465	9.951693	-0.057952	4.816003
282.789514	7999.978869	9.956698	-0.057932	4.816023
282.665380	7999.930675	9.961703	-0.057909	4.816010
282.906810	7999.967132	9.966707	-0.057954	4.816019
282.973265	7999.965145	9.971712	-0.057967	4.816018
282.847197	7999.900888	9.976717	-0.057944	4.816000
282.747154	7999.990975	9.981722	-0.057925	4.816027
282.688957	7999.876663	9.986727	-0.057914	4.815994
282.808479	7999.952575	9.991731	-0.057937	4.816015
282.942349	7999.956089	9.996736	-0.057962	4.816015
282.903171	7999.894480	10.001741	-0.057955	4.815998
283.032154	7999.932098	10.006746	-0.057979	4.816008
282.940374	7999.891972	10.011751	-0.057962	4.815997
283.049013	7999.926015	10.016755	-0.057982	4.816006
283.158045	7999.937625	10.021760	-0.058002	4.816009
282.928241	7999.900333	10.026765	-0.057960	4.815999
282.890438	7999.985140	10.031770	-0.057953	4.816024
282.850395	7999.945955	10.036775	-0.057945	4.816013
282.947081	7999.966957	10.041779	-0.057964	4.816019
282.854822	7999.973839	10.046784	-0.057947	4.816021
282.962166	7999.883907	10.051789	-0.057967	4.815994
283.137165	7999.948006	10.056794	-0.057999	4.816012
282.842558	7999.899919	10.061799	-0.057945	4.816000
283.005874	7999.941367	10.066803	-0.057975	4.816011
283.114546	7999.950833	10.071808	-0.057995	4.816013
282.989253	7999.942155	10.076813	-0.057972	4.816011
283.106125	7999.951770	10.081818	-0.057994	4.816013
283.054280	7999.954044	10.086823	-0.057985	4.816014
283.455693	7999.993411	10.091827	-0.058059	4.816024
283.325283	7999.979296	10.096832	-0.058035	4.816020
282.996558	7999.933793	10.101837	-0.057974	4.816009
283.263316	7999.994219	10.106842	-0.058024	4.816025
283.072422	7999.933057	10.111847	-0.057988	4.816008
282.966518	7999.953582	10.116851	-0.057969	4.816015
283.032318	7999.974023	10.121856	-0.057981	4.816020
283.098073	7999.977366	10.126861	-0.057994	4.816021
283.222082	7999.998866	10.131866	-0.058017	4.816026
283.101418	7999.925090	10.136871	-0.057994	4.816005
283.168550	7999.976543	10.141875	-0.058007	4.816020
283.072208	7999.982282	10.146880	-0.057989	4.816022
283.163041	7999.968984	10.151885	-0.058006	4.816018
283.431981	8000.004874	10.156890	-0.058056	4.816027
283.072658	7999.988734	10.161895	-0.057990	4.816024
283.119895	8000.020592	10.166899	-0.057999	4.816033
283.287481	7999.972359	10.171904	-0.058030	4.816018
283.217919	7999.961488	10.176909	-0.058017	4.816015
283.172970	8000.021589	10.181914	-0.058009	4.816033
283.170768	8000.002326	10.186919	-0.058008	4.816028
283.357012	8000.042055	10.191923	-0.058043	4.816038
283.395130	8000.037416	10.196928	-0.058051	4.816037
283.199509	7999.919534	10.201933	-0.058014	4.816003
283.273483	7999.992483	10.206938	-0.058028	4.816024
283.217678	7999.958353	10.211943	-0.058018	4.816015
283.398500	8000.012943	10.216947	-0.058052	4.816030
283.504265	8000.014878	10.221952	-0.058071	4.816030
283.538191	7999.942843	10.226957	-0.058078	4.816008
283.609125	7999.985818	10.231962	-0.058091	4.816020
283.452504	7999.953061	10.236967	-0.058062	4.816012
283.493350	7999.977323	10.241971	-0.058070	4.816019
283.440958	7999.978518	10.246976	-0.058060	4.816019
283.172799	7999.934116	10.251981	-0.058010	4.816008
283.316501	7999.950631	10.256986	-0.058037	4.816012
283.465861	7999.937329	10.261991	-0.058065	4.816007
283.313585	7999.950599	10.266995	-0.058037	4.816012
283.372113	7999.967703	10.272000	-0.058048	4.816016
283.571808	7999.959591	10.277005	-0.058085	4.816013
283.504080	8000.008592	10.282010	-0.058073	4.816028
283.173801	7999.987637	10.287015	-0.058011	4.816023
283.364458	8000.001801	10.292019	-0.058047	4.816026
283.259729	8000.000975	10.297024	-0.058027	4.816027
283.380067	8000.008517	10.302029	-0.058050	4.816028
283.407904	8000.021857	10.307034	-0.058055	4.816032
283.498950	7999.977576	10.312039	-0.058072	4.816019
283.475378	7999.985706	10.317043	-0.058068	4.816021
283.263617	8000.018197	10.322048	-0.058029	4.816032
283.347167	7999.989807	10.327053	-0.058044	4.816023
283.361674	8000.001836	10.332058	-0.058047	4.816026
283.183355	7999.933422	10.337063	-0.058014	4.816007
283.408932	7999.978140	10.342067	-0.058056	4.816019
283.596161	7999.968733	10.347072	-0.058091	4.816015
283.416019	7999.904560	10.352077	-0.058058	4.815998
283.403633	7999.957774	10.357082	-0.058056	4.816013
283.371559	7999.999944	10.362087	-0.058050	4.816026
283.429930	8000.009565	10.367091	-0.058061	4.816028
283.203409	7999.970193	10.372096	-0.058019	4.816018
283.393538	7999.880697	10.377101	-0.058054	4.815991
283.597825	8000.005171	10.382106	-0.058092	4.816026
283.319221	7999.988360	10.387111	-0.058041	4.816023
283.346445	7999.907656	10.392115	-0.058046	4.815999
283.659291	7999.959304	10.397120	-0.058104	4.816012
283.506887	7999.911663	10.402125	-0.058076	4.815999
283.475075	7999.998718	10.407130	-0.058070	4.816025
283.445713	7999.969343	10.412135	-0.058065	4.816016
283.447938	7999.957640	10.417139	-0.058065	4.816013
283.587867	7999.981567	10.422144	-0.058091	4.816019
283.534307	7999.957096	10.427149	-0.058081	4.816012
283.729523	7999.948902	10.432154	-0.058118	4.816009
283.544654	7999.917768	10.437159	-0.058084	4.816001
283.510428	7999.998368	10.442163	-0.058077	4.816025
283.524085	7999.983667	10.447168	-0.058080	4.816020
283.634561	7999.859596	10.452173	-0.058101	4.815983
283.647647	8000.038296	10.457178	-0.058103	4.816035
283.496882	8000.016330	10.462183	-0.058075	4.816030
283.786387	8000.037635	10.467187	-0.058129	4.816035
283.744695	8000.013379	10.472192	-0.058122	4.816028
283.686790	7999.950360	10.477197	-0.058111	4.816010
283.767496	8000.008473	10.482202	-0.058126	4.816026
283.648849	7999.942211	10.487207	-0.058104	4.816007
283.860089	7999.981327	10.492211	-0.058144	4.816018
283.758859	7999.991251	10.497216	-0.058125	4.816021
283.709465	7999.974334	10.502221	-0.058116	4.816016
283.573667	8000.017824	10.507226	-0.058091	4.816030
283.347037	7999.972039	10.512231	-0.058048	4.816018
283.679253	7999.998394	10.517235	-0.058110	4.816024
283.589089	7999.990354	10.522240	-0.058094	4.816022
283.690113	7999.962282	10.527245	-0.058113	4.816013
283.765138	8000.034183	10.532250	-0.058127	4.816034
283.502802	8000.002708	10.537255	-0.058078	4.816026
283.521111	8000.013738	10.542259	-0.058082	4.816029
283.550917	7999.988645	10.547264	-0.058087	4.816021
283.543321	7999.968215	10.552269	-0.058086	4.816015
283.685694	8000.019969	10.557274	-0.058113	4.816030
283.672848	7999.972729	10.562279	-0.058110	4.816016
283.625662	7999.998596	10.567283	-0.058102	4.816024
283.699601	7999.968963	10.572288	-0.058115	4.816015
283.690172	7999.948500	10.577293	-0.058114	4.816009
283.925154	7999.993390	10.582298	-0.058158	4.816021
283.815627	7999.918746	10.587303	-0.058137	4.816000
283.895326	7999.912726	10.592307	-0.058152	4.815997
283.856773	7999.956916	10.597312	-0.058145	4.816010
283.878862	7999.920997	10.602317	-0.058149	4.816000
283.884492	8000.021556	10.607322	-0.058151	4.816029
283.620802	7999.980439	10.612327	-0.058102	4.816019
283.794854	8000.008193	10.617331	-0.058134	4.816026
283.707647	7999.993795	10.622336	-0.058118	4.816022
283.661763	7999.932063	10.627341	-0.058110	4.816004
283.821571	7999.979860	10.632346	-0.058139	4.816017
283.645101	7999.967044	10.637351	-0.058107	4.816015
283.866902	7999.967883	10.642355	-0.058148	4.816014
283.717549	7999.991892	10.647360	-0.058120	4.816021
283.628493	7999.936854	10.652365	-0.058104	4.816006
283.721387	7999.985572	10.657370	-0.058121	4.816020
283.643981	7999.977763	10.662375	-0.058107	4.816018
283.866348	7999.951898	10.667379	-0.058149	4.816009
283.730572	8000.003937	10.672384	-0.058123	4.816025
283.763910	7999.920137	10.677389	-0.058130	4.816000
283.753096	8000.010780	10.682394	-0.058128	4.816027
283.810981	7999.934906	10.687399	-0.058139	4.816004
283.745251	7999.921967	10.692403	-0.058127	4.816001
283.683159	7999.940083	10.697408	-0.058115	4.816006
284.008190	7999.968446	10.702413	-0.058176	4.816013
284.031855	8000.021247	10.707418	-0.058180	4.816028
283.864437	8000.004321	10.712423	-0.058149	4.816024
283.946221	7999.941705	10.717427	-0.058165	4.816005
284.012406	7999.979251	10.722432	-0.058177	4.816016
283.762439	7999.909532	10.727437	-0.058131	4.815997
284.092077	8000.021328	10.732442	-0.058192	4.816028
283.935010	7999.988562	10.737447	-0.058163	4.816019
283.842844	7999.938810	10.742451	-0.058146	4.816005
283.829089	8000.016577	10.747456	-0.058143	4.816028
284.041141	7999.965947	10.752461	-0.058183	4.816012
284.115612	8000.016467	10.757466	-0.058197	4.816026
283.993260	7999.990744	10.762471	-0.058174	4.816020
284.144409	7999.922978	10.767475	-0.058203	4.815999
284.070270	8000.022086	10.772480	-0.058189	4.816028
283.831272	8000.022024	10.777485	-0.058145	4.816030
283.968042	7999.967888	10.782490	-0.058170	4.816013
283.947902	7999.946161	10.787495	-0.058166	4.816007
283.834756	7999.924880	10.792499	-0.058145	4.816001
283.971295	7999.981871	10.797504	-0.058171	4.816017
284.001763	8000.014493	10.802509	-0.058177	4.816026
283.974501	7999.991568	10.807514	-0.058172	4.816020
283.886867	7999.949379	10.812519	-0.058156	4.816008
284.008152	7999.918470	10.817523	-0.058178	4.815998
284.231581	7999.925751	10.822528	-0.058220	4.815999
284.065701	7999.948390	10.827533	-0.058189	4.816007
284.021195	7999.987129	10.832538	-0.058181	4.816018
284.161947	7999.948025	10.837543	-0.058207	4.816006
284.121561	7999.962261	10.842547	-0.058200	4.816010
284.048672	7999.996210	10.847552	-0.058187	4.816021
284.071446	7999.936794	10.852557	-0.058191	4.816003
284.092408	7999.983135	10.857562	-0.058195	4.816017
284.044047	7999.933112	10.862567	-0.058186	4.816002
284.130639	7999.963549	10.867571	-0.058202	4.816011
284.029402	8000.020490	10.872576	-0.058184	4.816028
283.962014	7999.889978	10.877581	-0.058171	4.815990
284.243956	8000.013729	10.882586	-0.058224	4.816025
284.197050	7999.974418	10.887591	-0.058215	4.816014
284.181756	7999.937819	10.892595	-0.058212	4.816003
283.997592	8000.019966	10.897600	-0.058178	4.816028
283.946135	7999.948514	10.902605	-0.058169	4.816007
284.214379	8000.018588	10.907610	-0.058219	4.816026
284.042340	8000.019744	10.912615	-0.058187	4.816028
284.080772	7999.977710	10.917619	-0.058194	4.816015
284.245767	7999.950802	10.922624	-0.058225	4.816006
284.190452	7999.963698	10.927629	-0.058215	4.816010
283.912219	8000.013145	10.932634	-0.058163	4.816026
283.995642	7999.998645	10.937639	-0.058179	4.816022
283.939627	7999.994431	10.942643	-0.058168	4.816021
284.024644	7999.988508	10.947648	-0.058184	4.816019
283.963480	7999.980995	10.952653	-0.058173	4.816017
284.134108	8000.028990	10.957658	-0.058205	4.816030
283.912321	7999.991840	10.962663	-0.058164	4.816020
284.168200	7999.986889	10.967667	-0.058211	4.816017
284.205644	8000.010021	10.972672	-0.058219	4.816024
283.939911	7999.953906	10.977677	-0.058169	4.816009
283.994150	7999.953835	10.982682	-0.058179	4.816009
284.105963	7999.956948	10.987687	-0.058200	4.816009
284.230585	7999.930374	10.992691	-0.058224	4.816000
284.086056	8000.005762	10.997696	-0.058197	4.816023
284.062941	7999.920935	11.002701	-0.058193	4.815999
284.285532	7999.980561	11.007706	-0.058234	4.816015
284.022201	7999.978987	11.012711	-0.058185	4.816016
284.102955	7999.993290	11.017715	-0.058200	4.816020
284.272935	7999.979296	11.022720	-0.058232	4.816015
283.918080	7999.929040	11.027725	-0.058166	4.816002
283.941277	7999.988244	11.032730	-0.058171	4.816019
283.969290	7999.951364	11.037735	-0.058176	4.816008
284.079370	7999.925594	11.042739	-0.058197	4.816000
284.092376	7999.947213	11.047744	-0.058199	4.816006
284.133810	7999.908440	11.052749	-0.058207	4.815995
284.297746	7999.974480	11.057754	-0.058238	4.816013
284.092770	7999.969693	11.062759	-0.058199	4.816013
283.987367	7999.944278	11.067763	-0.058180	4.816006
284.179499	7999.993732	11.072768	-0.058216	4.816019
284.136032	7999.914946	11.077773	-0.058208	4.815996
284.223972	7999.994563	11.082778	-0.058224	4.816019
283.984443	7999.966708	11.087783	-0.058180	4.816012
284.083187	7999.990955	11.092787	-0.058198	4.816019
284.039522	7999.961320	11.097792	-0.058190	4.816010
284.000378	7999.942453	11.102797	-0.058183	4.816005
284.277466	7999.948573	11.107802	-0.058235	4.816005
284.090704	7999.964420	11.112807	-0.058200	4.816011
283.918058	7999.951674	11.117811	-0.058168	4.816008
284.115406	7999.985194	11.122816	-0.058205	4.816017
284.162970	7999.998893	11.127821	-0.058214	4.816021
284.116704	8000.023709	11.132826	-0.058206	4.816028
284.023778	7999.981423	11.137831	-0.058188	4.816016
284.210655	7999.967736	11.142835	-0.058223	4.816011
284.279666	8000.006403	11.147840	-0.058236	4.816022
284.259930	7999.981477	11.152845	-0.058233	4.816015
284.412876	7999.999230	11.157850	-0.058261	4.816020
284.245933	7999.996204	11.162855	-0.058230	4.816020
284.286423	7999.920013	11.167859	-0.058238	4.815997
284.427842	7999.997398	11.172864	-0.058264	4.816019
284.294828	7999.874239	11.177869	-0.058240	4.815984
284.307853	7999.995237	11.182874	-0.058242	4.816019
284.444717	8000.011629	11.187879	-0.058268	4.816023
284.315516	8000.003946	11.192883	-0.058244	4.816021
284.190010	8000.033731	11.197888	-0.058221	4.816031
284.050405	7999.952127	11.202893	-0.058195	4.816008
284.371664	8000.010343	11.207898	-0.058255	4.816023
284.290306	8000.023834	11.212903	-0.058240	4.816027
284.097788	7999.992559	11.217907	-0.058204	4.816019
284.309938	8000.033830	11.222912	-0.058244	4.816030
284.314336	7999.947365	11.227917	-0.058244	4.816005
284.274747	7999.973371	11.232922	-0.058237	4.816013
284.326786	7999.943339	11.237927	-0.058247	4.816004
284.317447	7999.949591	11.242931	-0.058245	4.816005
284.375343	7999.975233	11.247936	-0.058256	4.816013
284.192046	7999.914206	11.252941	-0.058222	4.815996
284.345403	7999.978984	11.257946	-0.058251	4.816014
284.307284	7999.966547	11.262951	-0.058244	4.816010
284.040387	7999.958497	11.267955	-0.058194	4.816010
284.278987	7999.920105	11.272960	-0.058239	4.815997
284.224398	7999.905231	11.277965	-0.058229	4.815993
284.311347	7999.976282	11.282970	-0.058245	4.816013
284.428679	7999.996593	11.287975	-0.058267	4.816019
284.553497	7999.936896	11.292979	-0.058290	4.816000
284.327881	7999.983026	11.297984	-0.058248	4.816015
284.189661	7999.895036	11.302989	-0.058223	4.815990
284.371861	7999.960339	11.307994	-0.058257	4.816008
284.260104	7999.983963	11.312999	-0.058236	4.816016
284.293341	7999.981373	11.318003	-0.058242	4.816015
284.398911	8000.016430	11.323008	-0.058262	4.816025
284.371477	7999.945415	11.328013	-0.058257	4.816004
284.311039	7999.999893	11.333018	-0.058246	4.816020
284.256492	7999.973265	11.338023	-0.058236	4.816013
284.258413	8000.003231	11.343027	-0.058237	4.816021
284.307432	8000.050083	11.348032	-0.058246	4.816035
284.211891	7999.961800	11.353037	-0.058228	4.816010
284.238833	7999.991153	11.358042	-0.058233	4.816018
284.332319	7999.923407	11.363047	-0.058251	4.815998
284.299560	7999.861912	11.368051	-0.058245	4.815980
284.285782	7999.938610	11.373056	-0.058242	4.816002
284.516355	7999.880838	11.378061	-0.058285	4.815984
284.470924	7999.951617	11.383066	-0.058277	4.816005
284.432031	7999.943441	11.388071	-0.058270	4.816003
284.474411	7999.978417	11.393075	-0.058278	4.816013
284.392391	8000.008994	11.398080	-0.058263	4.816022
284.277943	7999.903269	11.403085	-0.058241	4.815992
284.609512	7999.934958	11.408090	-0.058303	4.816000
284.570697	7999.979144	11.413095	-0.058296	4.816013
284.197707	7999.960614	11.418099	-0.058227	4.816009
284.352718	8000.001914	11.423104	-0.058256	4.816020
284.330793	8000.018623	11.428109	-0.058252	4.816025
284.358226	7999.990281	11.433114	-0.058257	4.816017
284.199670	8000.016260	11.438119	-0.058228	4.816025
284.252820	7999.923202	11.443123	-0.058238	4.815998
284.370928	7999.969173	11.448128	-0.058260	4.816011
284.227312	7999.918485	11.453133	-0.058233	4.815997
284.166312	7999.946238	11.458138	-0.058222	4.816005
284.374693	7999.971411	11.463143	-0.058261	4.816011
284.422709	7999.938101	11.468147	-0.058270	4.816001
284.455438	7999.961147	11.473152	-0.058276	4.816008
284.309325	7999.920031	11.478157	-0.058249	4.815997
284.545939	7999.962816	11.483162	-0.058293	4.816008
284.541734	7999.961681	11.488167	-0.058292	4.816008
284.588635	7999.970026	11.493171	-0.058301	4.816010
284.516678	7999.999716	11.498176	-0.058288	4.816019
284.344784	7999.929279	11.503181	-0.058256	4.815999
284.558790	7999.964172	11.508186	-0.058296	4.816008
284.480284	7999.941383	11.513191	-0.058282	4.816002
284.457090	7999.931354	11.518195	-0.058277	4.815999
284.345726	7999.984905	11.523200	-0.058257	4.816015
284.364387	7999.977776	11.528205	-0.058260	4.816013
284.501902	8000.002729	11.533210	-0.058286	4.816020
284.389059	8000.007098	11.538215	-0.058265	4.816022
284.320893	7999.934273	11.543219	-0.058253	4.816001
284.409825	8000.029938	11.548224	-0.058269	4.816028
284.478795	8000.013038	11.553229	-0.058282	4.816023
284.588025	8000.020379	11.558234	-0.058303	4.816025
284.625095	7999.978320	11.563239	-0.058310	4.816012
284.641050	7999.943358	11.568243	-0.058313	4.816002
284.484814	8000.017465	11.573248	-0.058284	4.816024
284.494800	7999.951404	11.578253	-0.058286	4.816005
284.505962	7999.968716	11.583258	-0.058288	4.816010
284.378827	7999.969619	11.588263	-0.058264	4.816011
284.546753	7999.958794	11.593267	-0.058296	4.816007
284.686506	8000.017983	11.598272	-0.058322	4.816023
284.456377	7999.968925	11.603277	-0.058279	4.816010
284.553422	7999.977113	11.608282	-0.058297	4.816012
284.510420	7999.960313	11.613287	-0.058289	4.816007
284.411349	7999.899749	11.618291	-0.058271	4.815990
284.424138	7999.983342	11.623296	-0.058274	4.816015
284.626067	7999.905814	11.628301	-0.058311	4.815991
284.798361	7999.957046	11.633306	-0.058343	4.816005
284.482812	7999.986579	11.638311	-0.058285	4.816015
284.507550	7999.919719	11.643315	-0.058290	4.815995
284.641402	7999.973458	11.648320	-0.058315	4.816010
284.727493	7999.945114	11.653325	-0.058331	4.816002
284.672257	8000.047774	11.658330	-0.058321	4.816032
284.645617	8000.019516	11.663335	-0.058316	4.816024
284.686051	8000.026675	11.668339	-0.058323	4.816026
284.606500	8000.040198	11.673344	-0.058309	4.816030
284.502486	7999.925045	11.678349	-0.058289	4.815997
284.571725	7999.943413	11.683354	-0.058302	4.816002
284.562969	7999.977460	11.688359	-0.058301	4.816012
284.546048	7999.889538	11.693363	-0.058298	4.815986
284.729890	7999.934569	11.698368	-0.058332	4.815999
284.604660	7999.967565	11.703373	-0.058309	4.816009
284.665090	8000.025311	11.708378	-0.058320	4.816025
284.509580	8000.026767	11.713383	-0.058292	4.816027
284.709922	7999.923563	11.718387	-0.058329	4.815995
284.565708	7999.991477	11.723392	-0.058302	4.816016
284.435931	7999.901502	11.728397	-0.058278	4.815990
284.613160	7999.972059	11.733402	-0.058311	4.816010
284.834651	8000.016707	11.738407	-0.058353	4.816022
284.676192	7999.955061	11.743411	-0.058323	4.816005
284.723860	8000.036084	11.748416	-0.058332	4.816028
284.737540	7999.955130	11.753421	-0.058335	4.816005
284.594878	7999.976055	11.758426	-0.058308	4.816011
284.561314	7999.957289	11.763431	-0.058302	4.816006
284.555088	7999.919785	11.768435	-0.058301	4.815995
284.600515	8000.049923	11.773440	-0.058310	4.816033
284.554103	7999.989248	11.778445	-0.058301	4.816015
284.680665	8000.030031	11.783450	-0.058325	4.816027
284.561052	8000.037482	11.788455	-0.058303	4.816030
284.606871	7999.943222	11.793459	-0.058311	4.816002
284.795964	8000.022544	11.798464	-0.058347	4.816024
284.799191	7999.948880	11.803469	-0.058347	4.816002
284.817358	7999.985554	11.808474	-0.058351	4.816013
284.660191	8000.019037	11.813479	-0.058322	4.816024
284.588211	7999.920496	11.818483	-0.058308	4.815995
284.704960	8000.002776	11.823488	-0.058330	4.816019
284.633535	7999.992938	11.828493	-0.058317	4.816016
284.946190	8000.009324	11.833498	-0.058375	4.816019
284.858522	8000.006671	11.838503	-0.058359	4.816019
284.617757	7999.957420	11.843507	-0.058314	4.816006
284.715929	8000.010510	11.848512	-0.058333	4.816021
284.751659	7999.932094	11.853517	-0.058340	4.815998
284.756518	7999.953565	11.858522	-0.058341	4.816004
284.603673	8000.009568	11.863527	-0.058312	4.816021
284.640084	7999.976046	11.868531	-0.058319	4.816011
284.764430	7999.998623	11.873536	-0.058342	4.816017
284.670602	7999.944565	11.878541	-0.058325	4.816002
284.934210	7999.992117	11.883546	-0.058374	4.816014
284.799571	8000.033490	11.888551	-0.058349	4.816027
284.683911	7999.959800	11.893555	-0.058328	4.816006
284.747637	7999.973794	11.898560	-0.058340	4.816010
284.694718	7999.991008	11.903565	-0.058330	4.816015
284.642517	7999.937707	11.908570	-0.058321	4.816000
284.657877	8000.012799	11.913575	-0.058324	4.816022
284.855031	7999.989683	11.918579	-0.058360	4.816014
284.710969	7999.946465	11.923584	-0.058334	4.816002
284.466421	7999.982633	11.928589	-0.058288	4.816014
284.671804	8000.010959	11.933594	-0.058327	4.816021
284.568658	7999.999475	11.938599	-0.058307	4.816018
284.668375	7999.940391	11.943603	-0.058326	4.816000
284.751061	7999.971827	11.948608	-0.058342	4.816009
284.635326	7999.979349	11.953613	-0.058320	4.816012
284.765483	8000.003100	11.958618	-0.058345	4.816018
284.599720	7999.970174	11.963623	-0.058314	4.816010
284.755378	7999.901421	11.968627	-0.058343	4.815989
284.816010	7999.953828	11.973632	-0.058354	4.816004
284.543846	7999.930720	11.978637	-0.058304	4.815998
284.820125	7999.973159	11.983642	-0.058355	4.816009
284.728723	7999.974712	11.988647	-0.058338	4.816010
284.612939	7999.951244	11.993651	-0.058317	4.816004
284.771539	8000.044972	11.998656	-0.058347	4.816030
284.801644	7999.941876	12.003661	-0.058352	4.816000
284.810185	7999.996541	12.008666	-0.058354	4.816016
284.731810	8000.003675	12.013671	-0.058340	4.816019
284.772727	7999.985195	12.018675	-0.058347	4.816013
284.783436	8000.027076	12.023680	-0.058349	4.816025
284.699675	7999.971064	12.028685	-0.058334	4.816009
284.802588	7999.979359	12.033690	-0.058353	4.816011
284.771183	7999.972387	12.038695	-0.058347	4.816009
284.581929	7999.906976	12.043699	-0.058312	4.815991
284.595743	7999.952119	12.048704	-0.058315	4.816004
284.676902	7999.903383	12.053709	-0.058330	4.815990
284.851908	7999.927949	12.058714	-0.058363	4.815996
284.842539	7999.995112	12.063719	-0.058361	4.816015
284.871435	7999.915503	12.068723	-0.058367	4.815992
285.038325	8000.006177	12.073728	-0.058398	4.816018
284.841608	7999.947040	12.078733	-0.058361	4.816001
284.812273	7999.955066	12.083738	-0.058356	4.816004
284.822397	8000.014034	12.088743	-0.058358	4.816021
284.602159	7999.893560	12.093747	-0.058317	4.815987
284.641680	7999.907113	12.098752	-0.058325	4.815991
284.810310	7999.919810	12.103757	-0.058356	4.815994
284.784915	7999.924701	12.108762	-0.058351	4.815995
284.714717	7999.998237	12.113767	-0.058339	4.816017
284.603952	7999.918225	12.118771	-0.058318	4.815994
284.884748	8000.032342	12.123776	-0.058370	4.816026
284.678046	7999.981573	12.128781	-0.058332	4.816012
284.672674	7999.999652	12.133786	-0.058331	4.816018
284.951191	7999.979085	12.138791	-0.058383	4.816010
284.763268	7999.914766	12.143795	-0.058348	4.815992
284.711262	8000.022827	12.148800	-0.058339	4.816024
284.786212	7999.936577	12.153805	-0.058353	4.815999
284.787014	7999.986826	12.158810	-0.058353	4.816013
284.725843	7999.973969	12.163815	-0.058342	4.816010
284.813188	7999.984118	12.168819	-0.058358	4.816012
284.785237	7999.993238	12.173824	-0.058353	4.816015
284.779636	7999.994215	12.178829	-0.058352	4.816015
284.902107	8000.021033	12.183834	-0.058375	4.816023
284.818380	8000.037686	12.188839	-0.058360	4.816028
284.704239	7999.993945	12.193843	-0.058338	4.816016
284.716302	7999.948225	12.198848	-0.058341	4.816002
284.689089	7999.963770	12.203853	-0.058336	4.816007
284.945028	8000.001564	12.208858	-0.058384	4.816017
284.829716	7999.985585	12.213863	-0.058362	4.816013
284.912282	7999.998853	12.218867	-0.058378	4.816016
285.063311	8000.010161	12.223872	-0.058406	4.816019
284.880351	8000.017528	12.228877	-0.058372	4.816022
284.917413	7999.925245	12.233882	-0.058379	4.815995
285.007217	8000.033751	12.238887	-0.058396	4.816026
285.058443	7999.928902	12.243891	-0.058405	4.815995
284.983927	8000.001290	12.248896	-0.058392	4.816016
284.941871	7999.975958	12.253901	-0.058384	4.816009
285.105886	8000.012080	12.258906	-0.058415	4.816019
285.033390	8000.038556	12.263911	-0.058401	4.816027
284.696473	7999.983279	12.268915	-0.058339	4.816013
284.854530	8000.007538	12.273920	-0.058368	4.816019
284.847930	8000.017046	12.278925	-0.058367	4.816022
284.757590	8000.029305	12.283930	-0.058350	4.816026
284.689746	8000.006709	12.288935	-0.058338	4.816020
284.714256	7999.960148	12.293939	-0.058342	4.816006
284.888398	8000.029581	12.298944	-0.058375	4.816025
284.889170	7999.916334	12.303949	-0.058375	4.815992
284.900657	7999.975327	12.308954	-0.058377	4.816009
284.802811	8000.036604	12.313959	-0.058359	4.816028
284.842470	7999.995661	12.318963	-0.058367	4.816015
284.915882	8000.034409	12.323968	-0.058381	4.816026
284.712657	7999.985841	12.328973	-0.058343	4.816013
284.934552	8000.012330	12.333978	-0.058384	4.816020
284.797088	8000.052583	12.338983	-0.058359	4.816032
284.784927	8000.034207	12.343987	-0.058357	4.816027
284.881145	8000.054135	12.348992	-0.058375	4.816032
284.660656	8000.042653	12.353997	-0.058334	4.816030
284.823422	8000.076615	12.359002	-0.058364	4.816039
284.798865	8000.059081	12.364007	-0.058360	4.816034
284.928611	8000.058248	12.369011	-0.058384	4.816033
284.826281	8000.045710	12.374016	-0.058365	4.816030
284.566479	8000.001455	12.379021	-0.058317	4.816019
284.863206	7999.980150	12.384026	-0.058372	4.816011
284.855203	8000.031308	12.389031	-0.058371	4.816026
284.968625	8000.008805	12.394035	-0.058392	4.816019
285.021158	8000.039693	12.399040	-0.058402	4.816027
284.977691	8000.013266	12.404045	-0.058394	4.816020
285.064969	8000.042649	12.409050	-0.058410	4.816028
285.043212	8000.056156	12.414055	-0.058406	4.816032
284.860481	7999.983382	12.419059	-0.058372	4.816012
284.964659	8000.019484	12.424064	-0.058392	4.816022
284.906904	8000.025924	12.429069	-0.058381	4.816024
284.902299	8000.071801	12.434074	-0.058381	4.816037
284.925858	8000.027359	12.439079	-0.058385	4.816024
284.817623	8000.010440	12.444083	-0.058365	4.816020
284.910907	8000.030314	12.449088	-0.058382	4.816025
284.857253	7999.987673	12.454093	-0.058373	4.816013
284.739007	7999.979121	12.459098	-0.058351	4.816011
284.821749	8000.009489	12.464103	-0.058366	4.816020
284.829564	8000.024603	12.469107	-0.058368	4.816024
284.821879	8000.044777	12.474112	-0.058366	4.816030
284.945207	8000.021386	12.479117	-0.058390	4.816022
284.914853	7999.953522	12.484122	-0.058384	4.816003
284.966983	8000.039970	12.489127	-0.058394	4.816028
284.990950	7999.998742	12.494131	-0.058398	4.816015
285.036744	8000.039124	12.499136	-0.058407	4.816027
284.831404	7999.973419	12.504141	-0.058369	4.816009
284.964660	7999.957688	12.509146	-0.058394	4.816004
284.931602	8000.026557	12.514151	-0.058388	4.816024
284.736404	7999.982409	12.519155	-0.058352	4.816012
284.950414	8000.046156	12.524160	-0.058392	4.816030
284.763783	8000.002163	12.529165	-0.058357	4.816018
284.738276	8000.024151	12.534170	-0.058352	4.816024
284.784661	8000.037829	12.539175	-0.058361	4.816028
285.001338	8000.020411	12.544179	-0.058401	4.816022
285.048861	8000.030904	12.549184	-0.058410	4.816025
284.751193	8000.026566	12.554189	-0.058355	4.816025
284.803902	7999.984792	12.559194	-0.058365	4.816012
284.941272	8000.021498	12.564199	-0.058391	4.816022
284.820551	7999.963744	12.569203	-0.058368	4.816006
284.904719	8000.043295	12.574208	-0.058384	4.816029
284.886929	8000.038708	12.579213	-0.058381	4.816028
284.908775	7999.982480	12.584218	-0.058385	4.816011
284.886453	8000.030172	12.589223	-0.058381	4.816025
284.913018	7999.972961	12.594227	-0.058386	4.816008
285.148722	8000.043516	12.599232	-0.058430	4.816028
284.919521	7999.983787	12.604237	-0.058387	4.816011
284.902622	7999.986696	12.609242	-0.058384	4.816012
284.796538	8000.006149	12.614247	-0.058365	4.816019
284.874976	8000.001175	12.619251	-0.058380	4.816017
285.099898	8000.023446	12.624256	-0.058422	4.816022
284.951293	7999.916029	12.629261	-0.058394	4.815991
284.941714	7999.968227	12.634266	-0.058392	4.816007
284.858762	7999.980620	12.639271	-0.058377	4.816011
284.876252	7999.933931	12.644275	-0.058380	4.815997
285.162893	8000.009686	12.649280	-0.058434	4.816018
285.026137	7999.937748	12.654285	-0.058408	4.815997
285.023683	7999.960155	12.659290	-0.058408	4.816004
285.092679	8000.033019	12.664295	-0.058421	4.816025
284.892883	8000.030462	12.669299	-0.058384	4.816025
285.059461	8000.037779	12.674304	-0.058415	4.816026
285.044822	8000.008671	12.679309	-0.058412	4.816018
285.283180	8000.047215	12.684314	-0.058457	4.816028
285.033052	8000.060840	12.689319	-0.058411	4.816033
285.044793	8000.017251	12.694323	-0.058413	4.816020
285.273809	8000.044940	12.699328	-0.058456	4.816027
285.233872	7999.968352	12.704333	-0.058448	4.816005
285.258102	7999.942089	12.709338	-0.058453	4.815997
285.321518	8000.029812	12.714343	-0.058465	4.816023
285.052191	8000.004617	12.719347	-0.058415	4.816017
285.255700	8000.044664	12.724352	-0.058453	4.816027
285.227001	8000.050565	12.729357	-0.058448	4.816029
285.338462	7999.989556	12.734362	-0.058468	4.816011
285.093270	8000.029986	12.739367	-0.058423	4.816024
285.110250	8000.023894	12.744371	-0.058426	4.816022
285.234765	8000.050749	12.749376	-0.058449	4.816029
284.977608	8000.036462	12.754381	-0.058402	4.816026
285.020894	8000.052221	12.759386	-0.058410	4.816031
285.076927	8000.063938	12.764391	-0.058420	4.816034
285.136548	8000.060759	12.769395	-0.058432	4.816033
285.092064	8000.115529	12.774400	-0.058423	4.816049
284.974876	8000.021506	12.779405	-0.058402	4.816022
285.095453	7999.975623	12.784410	-0.058424	4.816008
285.065078	7999.996454	12.789415	-0.058419	4.816014
285.039017	7999.952177	12.794419	-0.058414	4.816001
285.245329	7999.999756	12.799424	-0.058452	4.816014
285.199856	8000.000008	12.804429	-0.058444	4.816015
285.124381	7999.979410	12.809434	-0.058430	4.816009
285.321273	8000.038572	12.814439	-0.058467	4.816025
285.043624	7999.981167	12.819443	-0.058415	4.816010
285.054411	8000.045491	12.824448	-0.058418	4.816029
285.122269	8000.001855	12.829453	-0.058430	4.816015
285.088963	7999.991642	12.834458	-0.058424	4.816013
285.126033	8000.046827	12.839463	-0.058431	4.816029
284.963177	8000.058835	12.844467	-0.058401	4.816033
285.100951	8000.062422	12.849472	-0.058427	4.816033
284.959389	8000.023523	12.854477	-0.058400	4.816023
285.043362	7999.934230	12.859482	-0.058416	4.815996
285.164807	8000.014460	12.864487	-0.058439	4.816019
285.053956	7999.973983	12.869491	-0.058418	4.816008
285.216766	8000.040005	12.874496	-0.058449	4.816026
285.158180	8000.006891	12.879501	-0.058438	4.816017
285.188645	7999.965781	12.884506	-0.058444	4.816005
285.435957	7999.998077	12.889511	-0.058490	4.816013
285.250677	7999.964794	12.894515	-0.058456	4.816004
285.315692	8000.015145	12.899520	-0.058468	4.816018
285.274635	8000.026163	12.904525	-0.058460	4.816022
285.394550	7999.945004	12.909530	-0.058483	4.815997
285.486865	7999.994783	12.914535	-0.058500	4.816011
285.349749	7999.995504	12.919539	-0.058475	4.816012
285.228340	8000.067040	12.924544	-0.058452	4.816034
285.218159	7999.969621	12.929549	-0.058450	4.816005
285.211012	7999.955610	12.934554	-0.058449	4.816001
285.320201	8000.056989	12.939559	-0.058470	4.816030
285.103534	8000.061605	12.944563	-0.058429	4.816033
285.310650	8000.096376	12.949568	-0.058468	4.816042
285.254508	8000.076130	12.954573	-0.058458	4.816036
285.222449	8000.024263	12.959578	-0.058452	4.816021
285.131080	8000.083522	12.964583	-0.058435	4.816039
284.891472	8000.018261	12.969587	-0.058390	4.816021
285.132546	8000.058992	12.974592	-0.058435	4.816032
284.963212	8000.013177	12.979597	-0.058404	4.816020
285.021052	7999.995005	12.984602	-0.058415	4.816014
285.166875	8000.034003	12.989607	-0.058442	4.816025
284.825250	7999.991463	12.994611	-0.058379	4.816014
285.084782	8000.043216	12.999616	-0.058427	4.816028
285.101796	8000.020027	13.004621	-0.058430	4.816021
285.270133	8000.048749	13.009626	-0.058462	4.816028
285.315287	8000.047444	13.014631	-0.058470	4.816028
285.191202	7999.985354	13.019635	-0.058447	4.816010
285.354083	8000.031074	13.024640	-0.058478	4.816023
285.273391	8000.026410	13.029645	-0.058463	4.816022
285.299514	8000.027965	13.034650	-0.058468	4.816022
285.393865	8000.020076	13.039655	-0.058485	4.816019
285.223495	7999.985996	13.044659	-0.058454	4.816010
285.493037	8000.051824	13.049664	-0.058504	4.816028
285.377732	8000.056148	13.054669	-0.058483	4.816030
285.305966	8000.061264	13.059674	-0.058470	4.816032
285.290714	8000.057791	13.064679	-0.058467	4.816031
285.303282	8000.024904	13.069683	-0.058469	4.816021
285.312916	8000.089207	13.074688	-0.058471	4.816040
285.115747	8000.054639	13.079693	-0.058435	4.816031
285.096931	8000.028661	13.084698	-0.058431	4.816023
285.124132	8000.059088	13.089703	-0.058436	4.816032
285.235350	7999.985251	13.094707	-0.058457	4.816010
285.168988	8000.048171	13.099712	-0.058445	4.816029
285.284898	7999.965871	13.104717	-0.058467	4.816004
285.240354	7999.992855	13.109722	-0.058458	4.816012
285.262432	8000.057385	13.114727	-0.058463	4.816031
285.465820	8000.004461	13.119731	-0.058501	4.816014
285.325924	7999.961318	13.124736	-0.058475	4.816002
285.258514	8000.009258	13.129741	-0.058462	4.816017
285.282766	7999.976583	13.134746	-0.058467	4.816007
285.447990	8000.011660	13.139751	-0.058498	4.816016
285.143556	7999.994374	13.144755	-0.058441	4.816013
285.107986	8000.002287	13.149760	-0.058435	4.816015
285.295361	7999.943728	13.154765	-0.058470	4.815997
285.214265	7999.904862	13.159770	-0.058455	4.815986
285.169699	8000.013060	13.164775	-0.058446	4.816018
285.349304	8000.033438	13.169779	-0.058480	4.816023
285.305314	8000.066844	13.174784	-0.058472	4.816033
285.116187	8000.039902	13.179789	-0.058437	4.816026
285.222610	8000.048262	13.184794	-0.058457	4.816028
285.238809	8000.085969	13.189799	-0.058460	4.816039
285.012318	8000.015603	13.194803	-0.058418	4.816020
285.302634	8000.074329	13.199808	-0.058472	4.816035
285.388576	8000.021405	13.204813	-0.058488	4.816020
285.364296	8000.022042	13.209818	-0.058484	4.816020
285.248861	8000.048805	13.214823	-0.058462	4.816028
285.260504	8000.025518	13.219827	-0.058465	4.816021
285.455720	8000.017327	13.224832	-0.058501	4.816018
285.209824	8000.004313	13.229837	-0.058455	4.816015
285.442886	7999.998949	13.234842	-0.058499	4.816013
285.357763	8000.010233	13.239847	-0.058483	4.816016
285.271035	8000.001185	13.244851	-0.058467	4.816014
285.301975	8000.018857	13.249856	-0.058473	4.816019
285.306957	8000.012547	13.254861	-0.058474	4.816017
285.401012	7999.999309	13.259866	-0.058492	4.816013
285.356431	8000.014538	13.264871	-0.058483	4.816018
285.226826	7999.950210	13.269875	-0.058459	4.816000
285.275250	7999.935073	13.274880	-0.058468	4.815995
285.184925	7999.950537	13.279885	-0.058452	4.816000
285.051361	7999.984450	13.284890	-0.058427	4.816010
285.200152	8000.043806	13.289895	-0.058455	4.816027
285.239954	8000.014620	13.294899	-0.058462	4.816018
285.249959	8000.040459	13.299904	-0.058464	4.816026
285.435070	8000.044908	13.304909	-0.058499	4.816026
285.326516	7999.969208	13.309914	-0.058479	4.816005
285.404078	8000.012307	13.314919	-0.058493	4.816017
285.118431	8000.024217	13.319923	-0.058440	4.816022
285.396963	8000.066699	13.324928	-0.058492	4.816033
285.250042	8000.039457	13.329933	-0.058465	4.816025
285.364770	8000.018047	13.334938	-0.058487	4.816019
285.521450	8000.091439	13.339943	-0.058516	4.816039
285.481187	8000.010570	13.344947	-0.058508	4.816016
285.263910	8000.099596	13.349952	-0.058468	4.816043
285.361411	8000.022303	13.354957	-0.058486	4.816020
285.453442	7999.958803	13.359962	-0.058504	4.816001
285.411820	8000.026448	13.364967	-0.058496	4.816021
285.299165	7999.925027	13.369971	-0.058475	4.815992
285.406438	7999.982558	13.374976	-0.058495	4.816008
285.236547	7999.983751	13.379981	-0.058464	4.816009
285.322918	7999.957550	13.384986	-0.058480	4.816001
285.415473	7999.998785	13.389991	-0.058497	4.816013
285.416870	7999.998821	13.394995	-0.058498	4.816013
285.365732	8000.045989	13.400000	-0.058488	4.816027
285.331169	8000.050714	13.405005	-0.058482	4.816028
285.435616	8000.069724	13.410010	-0.058501	4.816033
285.459183	8000.053065	13.415015	-0.058506	4.816028
285.505717	7999.986600	13.420019	-0.058515	4.816009
285.444153	8000.003657	13.425024	-0.058503	4.816014
285.432950	7999.995983	13.430029	-0.058501	4.816012
285.323640	7999.971563	13.435034	-0.058481	4.816005
285.517489	8000.039220	13.440039	-0.058517	4.816024
285.390048	7999.978137	13.445043	-0.058494	4.816007
285.299457	7999.979705	13.450048	-0.058477	4.816008
285.311023	8000.023739	13.455053	-0.058479	4.816020
285.498094	7999.991891	13.460058	-0.058514	4.816010
285.660426	8000.067523	13.465063	-0.058545	4.816031
285.377304	7999.979027	13.470067	-0.058492	4.816007
285.469017	8000.043757	13.475072	-0.058509	4.816025
285.506071	8000.005971	13.480077	-0.058516	4.816014
285.507966	7999.938693	13.485082	-0.058516	4.815995
285.395382	8000.048860	13.490087	-0.058496	4.816027
285.438069	7999.981256	13.495091	-0.058504	4.816007
285.422922	8000.045109	13.500096	-0.058501	4.816026
285.431190	8000.035652	13.505101	-0.058503	4.816023
285.614680	8000.009082	13.510106	-0.058537	4.816015
285.683631	7999.990044	13.515111	-0.058550	4.816009
285.389126	7999.965459	13.520115	-0.058495	4.816003
285.440106	7999.946094	13.525120	-0.058505	4.815997
285.662929	7999.961915	13.530125	-0.058546	4.816000
285.375152	7999.953482	13.535130	-0.058493	4.816000
285.628049	8000.022214	13.540135	-0.058540	4.816018
285.292744	7999.970170	13.545139	-0.058478	4.816005
285.630713	8000.067166	13.550144	-0.058541	4.816031
285.556196	8000.034830	13.555149	-0.058527	4.816022
285.580186	7999.919866	13.560154	-0.058532	4.815989
285.625148	8000.025421	13.565159	-0.058540	4.816019
285.445209	7999.948421	13.570163	-0.058507	4.815998
285.537037	8000.047348	13.575168	-0.058524	4.816026
285.318349	8000.038035	13.580173	-0.058483	4.816025
285.344753	7999.996850	13.585178	-0.058488	4.816012
285.367646	8000.052846	13.590183	-0.058493	4.816029
285.273732	7999.993442	13.595187	-0.058475	4.816012
285.429563	7999.980260	13.600192	-0.058504	4.816007
285.271969	8000.038313	13.605197	-0.058475	4.816025
285.336130	7999.950796	13.610202	-0.058487	4.815999
285.459596	8000.037476	13.615207	-0.058510	4.816024
285.355574	7999.984299	13.620211	-0.058491	4.816009
285.449487	8000.026627	13.625216	-0.058509	4.816020
285.575303	7999.943438	13.630221	-0.058532	4.815995
285.526792	7999.898753	13.635226	-0.058523	4.815983
285.416570	8000.000413	13.640231	-0.058503	4.816013
285.361704	7999.944926	13.645235	-0.058493	4.815997
285.478157	7999.999419	13.650240	-0.058515	4.816012
285.514912	7999.979795	13.655245	-0.058522	4.816006
285.581318	7999.931858	13.660250	-0.058534	4.815992
285.762930	8000.007841	13.665255	-0.058568	4.816013
285.562789	7999.946503	13.670259	-0.058531	4.815996
285.825618	8000.014347	13.675264	-0.058580	4.816015
285.695718	8000.004513	13.680269	-0.058556	4.816013
285.548763	7999.912084	13.685274	-0.058528	4.815986
285.601764	8000.003893	13.690279	-0.058539	4.816013
285.434406	7999.954906	13.695283	-0.058507	4.816000
285.498893	8000.013796	13.700288	-0.058520	4.816016
285.412090	8000.003678	13.705293	-0.058504	4.816014
285.476086	7999.933256	13.710298	-0.058516	4.815993
285.545905	8000.047812	13.715303	-0.058529	4.816026
285.581609	7999.991836	13.720307	-0.058535	4.816010
285.608091	7999.980574	13.725312	-0.058540	4.816006
285.521797	7999.997180	13.730317	-0.058525	4.816011
285.374218	7999.970995	13.735322	-0.058497	4.816005
285.594256	7999.958982	13.740327	-0.058538	4.816000
285.670700	7999.984962	13.745331	-0.058553	4.816007
285.713484	8000.054145	13.750336	-0.058561	4.816027
285.657429	8000.046723	13.755341	-0.058550	4.816025
285.445506	7999.975553	13.760346	-0.058511	4.816005
285.706614	8000.063670	13.765351	-0.058560	4.816030
285.480358	7999.978346	13.770355	-0.058518	4.816006
285.573676	7999.958683	13.775360	-0.058535	4.816000
285.658910	7999.988029	13.780365	-0.058551	4.816008
285.446071	7999.871961	13.785370	-0.058512	4.815975
285.646698	7999.979280	13.790375	-0.058549	4.816005
285.677286	7999.970230	13.795379	-0.058555	4.816003
285.765817	8000.000705	13.800384	-0.058571	4.816011
285.473902	8000.029598	13.805389	-0.058517	4.816021
285.399598	8000.003678	13.810394	-0.058504	4.816014
285.564515	8000.081495	13.815399	-0.058534	4.816036
285.439090	8000.020448	13.820403	-0.058511	4.816019
285.549196	8000.047041	13.825408	-0.058532	4.816026
285.450680	8000.060219	13.830413	-0.058514	4.816030
285.518122	7999.978105	13.835418	-0.058526	4.816006
285.477736	8000.022263	13.840423	-0.058519	4.816019
285.503036	8000.004568	13.845427	-0.058524	4.816014
285.637965	7999.989937	13.850432	-0.058549	4.816009
285.477078	7999.978470	13.855437	-0.058519	4.816006
285.599960	7999.947590	13.860442	-0.058542	4.815996
285.650016	8000.057512	13.865447	-0.058551	4.816028
285.522766	7999.979334	13.870451	-0.058528	4.816006
285.470478	7999.980530	13.875456	-0.058518	4.816007
285.648673	8000.037216	13.880461	-0.058551	4.816022
285.655576	7999.983921	13.885466	-0.058553	4.816007
285.821593	7999.986954	13.890471	-0.058584	4.816007
285.723600	7999.977701	13.895475	-0.058566	4.816005
285.858937	8000.026127	13.900480	-0.058591	4.816018
285.630871	8000.024123	13.905485	-0.058549	4.816019
285.779489	7999.930662	13.910490	-0.058576	4.815990
285.835642	8000.027872	13.915495	-0.058587	4.816019
285.503203	7999.987635	13.920499	-0.058525	4.816009
285.709754	7999.996749	13.925504	-0.058564	4.816010
285.902103	8000.036595	13.930509	-0.058600	4.816021
285.853932	7999.961993	13.935514	-0.058591	4.815999
285.690239	8000.026348	13.940519	-0.058561	4.816019
285.760874	8000.005203	13.945523	-0.058574	4.816012
285.836482	8000.052542	13.950528	-0.058588	4.816026
285.767763	8000.048096	13.955533	-0.058575	4.816025
285.633236	7999.967647	13.960538	-0.058550	4.816002
285.926652	8000.031775	13.965543	-0.058605	4.816019
285.769443	8000.009688	13.970547	-0.058576	4.816014
285.739936	8000.029465	13.975552	-0.058571	4.816020
285.677949	8000.070024	13.980557	-0.058559	4.816032
285.702687	7999.965760	13.985562	-0.058564	4.816001
285.703336	8000.044861	13.990567	-0.058564	4.816024
285.550300	7999.998272	13.995571	-0.058536	4.816011
285.747028	8000.014688	14.000576	-0.058572	4.816015
285.812135	8000.015884	14.005581	-0.058585	4.816015
285.683256	7999.931264	14.010586	-0.058561	4.815991
285.797939	8000.004961	14.015591	-0.058582	4.816012
285.783664	7999.961966	14.020595	-0.058580	4.816000
285.707770	7999.963801	14.025600	-0.058566	4.816000
285.685601	7999.990124	14.030605	-0.058562	4.816008
285.796422	7999.954750	14.035610	-0.058582	4.815997
285.734004	7999.991027	14.040615	-0.058571	4.816008
285.562620	7999.969751	14.045619	-0.058539	4.816003
285.736133	7999.994293	14.050624	-0.058571	4.816009
285.781196	8000.003674	14.055629	-0.058580	4.816012
285.586893	7999.988392	14.060634	-0.058544	4.816008
285.728181	8000.058299	14.065639	-0.058570	4.816028
285.680639	7999.991189	14.070643	-0.058562	4.816009
285.820269	8000.010840	14.075648	-0.058588	4.816014
285.992012	8000.047106	14.080653	-0.058620	4.816023
285.870453	7999.936971	14.085658	-0.058597	4.815992
285.765009	7999.990631	14.090663	-0.058578	4.816008
285.534259	8000.021706	14.095667	-0.058535	4.816018
285.667901	8000.030561	14.100672	-0.058560	4.816020
285.539457	8000.038920	14.105677	-0.058536	4.816023
285.586264	7999.946812	14.110682	-0.058545	4.815996
285.772475	8000.033566	14.115687	-0.058580	4.816020
285.473569	7999.986459	14.120691	-0.058524	4.816008
285.545753	7999.971754	14.125696	-0.058538	4.816004
285.600588	8000.011234	14.130701	-0.058548	4.816015
285.710608	7999.942718	14.135706	-0.058569	4.815994
285.723816	8000.011362	14.140711	-0.058571	4.816014
285.613642	7999.986926	14.145715	-0.058551	4.816008
285.735293	7999.985945	14.150720	-0.058574	4.816007
285.999338	8000.050607	14.155725	-0.058623	4.816024
285.663113	7999.947251	14.160730	-0.058560	4.815996
285.675221	8000.008394	14.165735	-0.058563	4.816014
285.779912	7999.905585	14.170739	-0.058582	4.815983
285.802315	7999.936994	14.175744	-0.058587	4.815992
285.628741	8000.009717	14.180749	-0.058554	4.816014
285.671166	7999.949589	14.185754	-0.058562	4.815996
285.966516	8000.007339	14.190759	-0.058617	4.816012
285.552240	7999.988053	14.195763	-0.058540	4.816008
285.702797	8000.014315	14.200768	-0.058569	4.816015
285.851944	7999.987119	14.205773	-0.058596	4.816006
285.652035	7999.941814	14.210778	-0.058559	4.815994
285.831027	8000.010270	14.215783	-0.058593	4.816013
285.894611	7999.937702	14.220787	-0.058605	4.815992
285.901315	7999.956002	14.225792	-0.058606	4.815997
285.807903	8000.045146	14.230797	-0.058589	4.816024
285.880148	7999.960981	14.235802	-0.058602	4.815999
285.823929	7999.303842	14.240807	-0.058592	4.815807

285.794237	7995.993157	14.245811	-0.058584	4.814840
285.664897	7990.583624	14.250816	-0.058557	4.813259
285.587001	7983.941581	14.255821	-0.058538	4.811318
285.462468	7976.597124	14.260826	-0.058510	4.809170
285.661867	7969.031261	14.265831	-0.058542	4.806955
285.439950	7961.149179	14.270835	-0.058496	4.804649
285.338590	7953.404097	14.275840	-0.058472	4.802380
285.361664	7945.444349	14.280845	-0.058471	4.800048
285.313327	7937.475569	14.285850	-0.058457	4.797711
285.414199	7929.443996	14.290855	-0.058471	4.795355
285.161351	7921.409515	14.295859	-0.058419	4.792998
285.306532	7913.368489	14.300864	-0.058441	4.790636
285.381358	7905.420572	14.305869	-0.058449	4.788301
285.241687	7897.334031	14.310874	-0.058418	4.785925
285.203051	7889.445249	14.315879	-0.058406	4.783605
285.068954	7881.390175	14.320883	-0.058376	4.781236
285.142221	7873.461047	14.325888	-0.058385	4.778902
285.025495	7865.413177	14.330893	-0.058358	4.776532
285.067438	7857.406648	14.335898	-0.058360	4.774173
285.123415	7849.379921	14.340903	-0.058366	4.771806
284.872904	7841.373936	14.345907	-0.058314	4.769446
284.839670	7833.394129	14.350912	-0.058303	4.767091
284.897961	7825.410047	14.355917	-0.058308	4.764734
284.797012	7817.442506	14.360922	-0.058285	4.762381
284.660489	7809.377079	14.365927	-0.058254	4.759998
284.701037	7801.409955	14.370931	-0.058256	4.757642
284.580586	7793.363410	14.375936	-0.058229	4.755262
284.522976	7785.356563	14.380941	-0.058213	4.752893
284.528348	7777.327140	14.385946	-0.058209	4.750515
284.675816	7769.343562	14.390951	-0.058231	4.748149
284.495172	7761.331424	14.395955	-0.058193	4.745775
284.442934	7753.369140	14.400960	-0.058178	4.743414
284.441422	7745.337823	14.405965	-0.058172	4.741031
284.222473	7737.348994	14.410970	-0.058126	4.738660
284.192962	7729.330723	14.415975	-0.058116	4.736278
284.055235	7721.377240	14.420979	-0.058085	4.733915
284.136838	7713.296924	14.425984	-0.058095	4.731513
284.170655	7705.336630	14.430989	-0.058096	4.729144
283.984795	7697.287754	14.435994	-0.058057	4.726750
284.199079	7689.331140	14.440999	-0.058091	4.724380
283.931387	7681.338849	14.446003	-0.058037	4.721999
284.114893	7673.306098	14.451008	-0.058066	4.719605
284.154673	7665.378488	14.456013	-0.058068	4.717240
283.857228	7657.323906	14.461018	-0.058007	4.714838
283.901188	7649.317621	14.466023	-0.058010	4.712448
283.777484	7641.264690	14.471027	-0.057982	4.710043
283.759517	7633.301509	14.476032	-0.057974	4.707663
283.826619	7625.262756	14.481037	-0.057981	4.705260
283.796059	7617.342004	14.486042	-0.057970	4.702890
283.948445	7609.338203	14.491047	-0.057994	4.700494
283.745686	7601.334382	14.496051	-0.057951	4.698098
283.455356	7593.290251	14.501056	-0.057892	4.695689
283.656293	7585.314731	14.506061	-0.057924	4.693298
283.517936	7577.241662	14.511066	-0.057893	4.690877
283.435545	7569.316800	14.516071	-0.057873	4.688499
283.223049	7561.325366	14.521075	-0.057828	4.686101
283.310043	7553.314321	14.526080	-0.057839	4.683694
283.413402	7545.328256	14.531085	-0.057853	4.681294
283.213677	7537.310944	14.536090	-0.057811	4.678884
283.184803	7529.305221	14.541095	-0.057801	4.676476
283.165435	7521.195857	14.546099	-0.057792	4.674035
283.086435	7513.162919	14.551104	-0.057772	4.671616
283.264387	7505.212411	14.556109	-0.057800	4.669220
283.222146	7497.223203	14.561114	-0.057787	4.666812
282.996990	7489.211224	14.566119	-0.057740	4.664396
283.007996	7481.293750	14.571123	-0.057737	4.662006
282.973631	7473.225031	14.576128	-0.057725	4.659570
282.947612	7465.272185	14.581133	-0.057716	4.657168
282.865748	7457.218883	14.586138	-0.057695	4.654734
282.885071	7449.252886	14.591143	-0.057694	4.652325
282.689105	7441.179653	14.596147	-0.057652	4.649883
282.741171	7433.244835	14.601152	-0.057657	4.647481
282.809120	7425.241006	14.606157	-0.057664	4.645056
282.763029	7417.236765	14.611162	-0.057650	4.642631
282.776035	7409.226661	14.616167	-0.057648	4.640202
282.624403	7401.278812	14.621171	-0.057614	4.637792
282.603933	7393.199864	14.626176	-0.057606	4.635340
282.696648	7385.186208	14.631181	-0.057618	4.632906
282.551451	7377.128769	14.636186	-0.057586	4.630458
282.613838	7369.246675	14.641191	-0.057592	4.628062
282.405973	7361.175017	14.646195	-0.057548	4.625607
282.362582	7353.207617	14.651200	-0.057535	4.623182
282.191220	7345.237988	14.656205	-0.057498	4.620756
281.998250	7337.184465	14.661210	-0.057457	4.618303
282.098032	7329.202399	14.666215	-0.057471	4.615870
282.028903	7321.148499	14.671219	-0.057453	4.613414
282.192980	7313.135059	14.676224	-0.057478	4.610969
282.143307	7305.196095	14.681229	-0.057464	4.608545
282.001395	7297.128399	14.686234	-0.057432	4.606081
281.939063	7289.213239	14.691239	-0.057415	4.603662
282.000425	7281.167613	14.696243	-0.057422	4.601202
281.871679	7273.245552	14.701248	-0.057393	4.598778
281.814455	7265.203344	14.706253	-0.057377	4.596316
281.746283	7257.137959	14.711258	-0.057359	4.593846
281.602361	7249.105478	14.716263	-0.057327	4.591385
281.592553	7241.101756	14.721267	-0.057320	4.588931
281.616431	7233.099258	14.726272	-0.057320	4.586476
281.479766	7225.186580	14.731277	-0.057289	4.584048
281.360904	7217.127717	14.736282	-0.057262	4.581573
281.311601	7209.150388	14.741287	-0.057247	4.579122
281.414069	7201.156854	14.746291	-0.057261	4.576664
281.296478	7193.153706	14.751296	-0.057234	4.574203
281.171341	7185.106252	14.756301	-0.057206	4.571726
281.331738	7177.089031	14.761306	-0.057231	4.569257
281.131495	7169.144717	14.766311	-0.057188	4.566810
280.925896	7161.121734	14.771315	-0.057145	4.564336
281.096974	7153.136661	14.776320	-0.057172	4.561874
281.130294	7145.146096	14.781325	-0.057173	4.559408
280.825609	7137.168905	14.786330	-0.057111	4.556945
281.097690	7129.159026	14.791335	-0.057157	4.554471
281.086134	7121.138169	14.796339	-0.057149	4.551991
280.956638	7113.100908	14.801344	-0.057120	4.549506
280.855321	7105.141630	14.806349	-0.057096	4.547043
280.743727	7097.086947	14.811354	-0.057070	4.544549
280.702973	7089.137208	14.816359	-0.057058	4.542086
280.600039	7081.063170	14.821363	-0.057033	4.539584
280.668616	7073.141829	14.826368	-0.057041	4.537127
280.667848	7065.152654	14.831373	-0.057036	4.534648
280.507942	7057.091210	14.836378	-0.057001	4.532145
280.717645	7049.088706	14.841383	-0.057035	4.529660
280.586397	7041.095309	14.846387	-0.057005	4.527176
280.236434	7033.075426	14.851392	-0.056935	4.524681
280.231474	7025.168523	14.856397	-0.056929	4.522221
280.098316	7017.144359	14.861402	-0.056899	4.519723
280.003369	7009.176570	14.866407	-0.056876	4.517241
279.849953	7001.109414	14.871411	-0.056843	4.514726
280.071242	6993.015400	14.876416	-0.056879	4.512203
280.191746	6985.063548	14.881421	-0.056896	4.509722
279.896285	6977.040867	14.886426	-0.056836	4.507217
279.869588	6969.071858	14.891431	-0.056826	4.504728
279.779410	6961.103733	14.896435	-0.056804	4.502237
279.693547	6953.040216	14.901440	-0.056783	4.499716
279.738614	6945.136889	14.906445	-0.056786	4.497243
279.489307	6937.078665	14.911450	-0.056735	4.494720
279.402552	6929.060649	14.916455	-0.056713	4.492208
279.536850	6921.037391	14.921459	-0.056733	4.489694
279.342664	6913.077063	14.926464	-0.056692	4.487197
279.509767	6905.067430	14.931469	-0.056718	4.484685
279.445108	6897.076184	14.936474	-0.056701	4.482176
279.400697	6889.048524	14.941479	-0.056687	4.479654
279.497886	6881.088670	14.946483	-0.056701	4.477153
279.334312	6873.072141	14.951488	-0.056665	4.474632
279.502998	6865.066962	14.956493	-0.056691	4.472113
279.104552	6857.043981	14.961498	-0.056612	4.469586
279.159108	6849.034096	14.966503	-0.056617	4.467064
279.012367	6841.028776	14.971507	-0.056585	4.464540
279.116428	6833.059117	14.976512	-0.056599	4.462027
279.257331	6825.087593	14.981517	-0.056620	4.459512
279.203585	6817.024725	14.986522	-0.056605	4.456967
279.015363	6809.051940	14.991527	-0.056565	4.454448
279.129761	6801.003372	14.996531	-0.056581	4.451904
279.025142	6793.014142	15.001536	-0.056556	4.449377
279.021841	6785.007625	15.006541	-0.056551	4.446844
278.911121	6777.009891	15.011546	-0.056525	4.444311
278.886598	6769.056139	15.016551	-0.056515	4.441791
278.683611	6760.997803	15.021555	-0.056472	4.439236
278.605457	6753.022377	15.026560	-0.056453	4.436706
278.662888	6745.014445	15.031565	-0.056458	4.434165
278.601675	6736.974253	15.036570	-0.056442	4.431612
278.580827	6728.988310	15.041575	-0.056433	4.429075
278.613773	6720.992514	15.046579	-0.056434	4.426533
278.582334	6712.978605	15.051584	-0.056423	4.423984
278.490345	6705.033895	15.056589	-0.056401	4.421455
278.431334	6696.970809	15.061594	-0.056384	4.418888
278.422682	6688.973457	15.066599	-0.056378	4.416339
278.156792	6681.012727	15.071603	-0.056323	4.413800
278.065026	6672.959312	15.076608	-0.056301	4.411231
278.174139	6665.013349	15.081613	-0.056316	4.408695
277.956222	6656.969194	15.086618	-0.056270	4.406125
277.951890	6648.995037	15.091623	-0.056265	4.403577
277.967339	6640.960784	15.096627	-0.056262	4.401008
278.024686	6632.984244	15.101632	-0.056268	4.398457
277.959545	6625.003476	15.106637	-0.056251	4.395902
277.728520	6616.984167	15.111642	-0.056203	4.393332
277.789518	6608.960177	15.116647	-0.056209	4.390761
277.759070	6600.985154	15.121651	-0.056198	4.388203
277.685121	6592.961032	15.126656	-0.056179	4.385628
277.953874	6584.996329	15.131661	-0.056224	4.383072
277.932597	6576.975876	15.136666	-0.056215	4.380496
277.849673	6569.023334	15.141671	-0.056195	4.377939
277.659011	6561.006462	15.146675	-0.056154	4.375360
277.529894	6552.980739	15.151680	-0.056125	4.372776
277.704888	6544.984597	15.156685	-0.056152	4.370203
277.401924	6536.972418	15.161690	-0.056091	4.367619
277.504307	6528.935659	15.166695	-0.056105	4.365029
277.523972	6521.006712	15.171699	-0.056103	4.362471
277.351287	6513.003705	15.176704	-0.056066	4.359887
277.384919	6505.028802	15.181709	-0.056067	4.357312
277.386692	6496.964546	15.186714	-0.056062	4.354706
277.304537	6488.904763	15.191719	-0.056042	4.352100
277.316464	6480.888589	15.196723	-0.056039	4.349506
277.362661	6472.909324	15.201728	-0.056043	4.346923
277.452541	6464.957074	15.206733	-0.056054	4.344348
277.389283	6456.984567	15.211738	-0.056037	4.341764
277.245507	6449.000139	15.216743	-0.056006	4.339173
277.154147	6440.965643	15.221747	-0.055983	4.336565
276.993331	6432.939341	15.226752	-0.055948	4.333958
277.115653	6424.962157	15.231757	-0.055966	4.331367
277.137478	6416.947599	15.236762	-0.055965	4.328762
277.179518	6408.950880	15.241767	-0.055968	4.326161
276.763860	6400.987679	15.246771	-0.055885	4.323566
276.784108	6392.944555	15.251776	-0.055884	4.320947
276.825978	6385.011200	15.256781	-0.055887	4.318362
276.778869	6376.953363	15.261786	-0.055873	4.315734
276.835007	6368.925967	15.266791	-0.055878	4.313115
276.713375	6360.939815	15.271795	-0.055850	4.310507
276.591005	6352.909844	15.276800	-0.055822	4.307883
276.642956	6344.918189	15.281805	-0.055827	4.305271
276.645207	6336.957294	15.286810	-0.055822	4.302668
276.667962	6328.946403	15.291815	-0.055821	4.300046
276.505146	6320.975124	15.296819	-0.055786	4.297435
276.305512	6312.901980	15.301824	-0.055744	4.294788
276.582319	6304.926610	15.306829	-0.055790	4.292175
276.130177	6296.900738	15.311834	-0.055701	4.289538
276.362511	6288.914241	15.316839	-0.055739	4.286918
276.212763	6280.952075	15.321843	-0.055706	4.284302
276.043757	6272.930732	15.326848	-0.055669	4.281664
276.036254	6264.957006	15.331853	-0.055663	4.279042
275.939048	6256.930616	15.336858	-0.055640	4.276399
276.157899	6248.904315	15.341863	-0.055675	4.273758
276.129486	6240.864387	15.346867	-0.055665	4.271109
276.120540	6232.876314	15.351872	-0.055658	4.268475
276.102210	6224.889633	15.356877	-0.055650	4.265840
275.801432	6216.926405	15.361882	-0.055589	4.263209
275.739995	6208.897860	15.366887	-0.055572	4.260557
275.838356	6200.925004	15.371891	-0.055585	4.257922
275.673640	6192.897812	15.376896	-0.055549	4.255266
275.470604	6184.921033	15.381901	-0.055507	4.252624
275.533915	6176.842386	15.386906	-0.055513	4.249950
275.576070	6168.947389	15.391911	-0.055516	4.247334
275.369079	6160.887871	15.396915	-0.055472	4.244660
275.439740	6152.962460	15.401920	-0.055480	4.242031
275.408373	6144.920606	15.406925	-0.055469	4.239362
275.243755	6136.955123	15.411930	-0.055434	4.236714
275.229295	6128.910754	15.416935	-0.055426	4.234040
275.186323	6120.883530	15.421939	-0.055413	4.231370
275.316177	6112.865021	15.426944	-0.055432	4.228702
275.163155	6104.932567	15.431949	-0.055398	4.226059
275.160971	6096.936257	15.436954	-0.055393	4.223395
275.223423	6088.930994	15.441959	-0.055399	4.220726
274.941570	6080.979930	15.446963	-0.055342	4.218070
275.096001	6072.885860	15.451968	-0.055365	4.215370
274.978016	6064.943099	15.456973	-0.055338	4.212715
274.924348	6056.872812	15.461978	-0.055323	4.210017
274.839227	6048.979398	15.466983	-0.055302	4.207375
274.971574	6040.944673	15.471987	-0.055322	4.204687
274.898406	6032.951920	15.476992	-0.055303	4.202010
274.721490	6024.989764	15.481997	-0.055265	4.199339
274.670605	6016.947979	15.487002	-0.055250	4.196642
274.757735	6008.875572	15.492007	-0.055262	4.193934
274.690689	6000.795412	15.497011	-0.055244	4.191220
274.400341	5992.853723	15.502016	-0.055185	4.188548
274.549964	5984.875738	15.507021	-0.055208	4.185868
274.441942	5976.878381	15.512026	-0.055182	4.183176
274.336008	5968.905625	15.517031	-0.055158	4.180491
274.302781	5960.923703	15.522035	-0.055146	4.177801
274.233608	5952.882349	15.527040	-0.055128	4.175090
274.232586	5944.935674	15.532045	-0.055123	4.172409
274.225281	5936.852846	15.537050	-0.055116	4.169681
274.288655	5928.906092	15.542055	-0.055123	4.166998
274.260733	5920.927704	15.547059	-0.055113	4.164301
274.263632	5912.931344	15.552064	-0.055108	4.161597
274.277584	5904.927835	15.557069	-0.055106	4.158888
274.072320	5896.906394	15.562074	-0.055062	4.156170
274.014940	5888.886284	15.567079	-0.055047	4.153451
274.004314	5880.861604	15.572083	-0.055040	4.150730
273.769096	5872.880129	15.577088	-0.054991	4.148019
273.632370	5864.895118	15.582093	-0.054960	4.145307
273.625371	5856.904541	15.587098	-0.054954	4.142592
273.831583	5848.881600	15.592103	-0.054987	4.139866
273.629271	5840.907322	15.597107	-0.054944	4.137151
273.595481	5832.839008	15.602112	-0.054933	4.134404
273.823535	5824.863136	15.607117	-0.054970	4.131690
273.586587	5816.859301	15.612122	-0.054921	4.128959
273.422770	5808.867434	15.617127	-0.054885	4.126231
273.472278	5800.930047	15.622131	-0.054890	4.123522
273.476818	5792.906264	15.627136	-0.054885	4.120782
273.538111	5784.955186	15.632141	-0.054892	4.118065
273.476366	5776.902446	15.637146	-0.054875	4.115310
273.504595	5768.861899	15.642151	-0.054875	4.112559
273.258526	5760.866806	15.647155	-0.054824	4.109817
273.184866	5752.849889	15.652160	-0.054805	4.107069
273.192671	5744.866315	15.657165	-0.054802	4.104331
273.047227	5736.871924	15.662170	-0.054770	4.101586
272.968716	5728.901364	15.667175	-0.054750	4.098848
272.971383	5720.918597	15.672179	-0.054745	4.096105
272.997877	5712.894904	15.677184	-0.054745	4.093347
272.838376	5704.897259	15.682189	-0.054710	4.090593
272.677252	5696.914200	15.687194	-0.054675	4.087842
272.633970	5688.915779	15.692199	-0.054662	4.085086
272.717517	5680.961358	15.697203	-0.054672	4.082344
272.832936	5672.927801	15.702208	-0.054689	4.079574
272.731501	5664.972257	15.707213	-0.054665	4.076826
272.659520	5656.909865	15.712218	-0.054646	4.074040
272.575385	5648.913986	15.717223	-0.054626	4.071274
272.598383	5640.931089	15.722227	-0.054625	4.068513
272.447689	5632.887465	15.727232	-0.054592	4.065726
272.391911	5624.963665	15.732237	-0.054576	4.062980
272.427169	5616.920975	15.737242	-0.054578	4.060193
272.483292	5608.942340	15.742247	-0.054583	4.057426
272.388007	5600.921302	15.747251	-0.054560	4.054640
272.224360	5592.925667	15.752256	-0.054524	4.051860
272.215896	5584.941838	15.757261	-0.054518	4.049085
272.051873	5576.911549	15.762266	-0.054482	4.046289
272.059940	5568.957804	15.767271	-0.054479	4.043520
272.158294	5560.942165	15.772275	-0.054492	4.040729
271.930676	5552.937514	15.777280	-0.054444	4.037936
271.772071	5544.938309	15.782285	-0.054410	4.035143
271.771886	5536.820056	15.787290	-0.054404	4.032309
271.838118	5528.857495	15.792295	-0.054412	4.029529
271.926574	5520.900362	15.797299	-0.054423	4.026749
271.698605	5512.883636	15.802304	-0.054376	4.023941
271.714177	5504.926398	15.807309	-0.054373	4.021156
271.666437	5496.929278	15.812314	-0.054359	4.018354
271.497679	5488.896684	15.817319	-0.054323	4.015536
271.384961	5480.901188	15.822323	-0.054297	4.012729
271.412967	5472.857209	15.827328	-0.054297	4.009906
271.371811	5464.924973	15.832333	-0.054284	4.007119
271.330429	5456.877544	15.837338	-0.054271	4.004290
271.276591	5448.923323	15.842343	-0.054256	4.001491
271.378631	5440.947403	15.847347	-0.054270	3.998685
271.194507	5432.918897	15.852352	-0.054231	3.995854
271.329004	5424.913803	15.857357	-0.054251	3.993034
271.087043	5416.897587	15.862362	-0.054200	3.990202
271.186562	5408.915986	15.867367	-0.054214	3.987386
271.008970	5400.892455	15.872371	-0.054176	3.984549
271.015247	5392.911388	15.877376	-0.054172	3.981728
270.940822	5384.918493	15.882381	-0.054153	3.978899
270.883790	5376.941102	15.887386	-0.054137	3.976074
270.876781	5368.945967	15.892391	-0.054131	3.973241
270.859112	5360.920064	15.897395	-0.054122	3.970395
270.861664	5352.910427	15.902400	-0.054118	3.967554
270.960965	5344.931031	15.907405	-0.054131	3.964722
270.726554	5336.965895	15.912410	-0.054082	3.961889
270.703782	5328.998371	15.917415	-0.054073	3.959055
270.722799	5320.992492	15.922419	-0.054071	3.956207
270.594808	5312.952015	15.927424	-0.054042	3.953342
270.583110	5304.956561	15.932429	-0.054035	3.950493
270.453812	5296.922620	15.937434	-0.054006	3.947626
270.428191	5288.930707	15.942439	-0.053996	3.944774
270.393615	5280.997461	15.947443	-0.053985	3.941940
270.346299	5272.976239	15.952448	-0.053971	3.939073
270.222522	5265.011722	15.957453	-0.053943	3.936223
270.238673	5256.956389	15.962458	-0.053940	3.933340
270.253808	5248.944481	15.967463	-0.053938	3.930471
270.069355	5241.010060	15.972467	-0.053899	3.927624
270.002998	5232.957311	15.977472	-0.053881	3.924735
270.131380	5225.007825	15.982477	-0.053900	3.921884
269.919935	5216.993222	15.987482	-0.053856	3.919001
269.937009	5208.981014	15.992487	-0.053854	3.916121
269.996136	5201.012499	15.997491	-0.053860	3.913256
269.826289	5192.969431	16.002496	-0.053823	3.910357
269.841280	5185.006231	16.007501	-0.053821	3.907489
269.718335	5176.945938	16.012506	-0.053793	3.904581
269.635800	5168.979612	16.017511	-0.053772	3.901705
269.646511	5161.004062	16.022515	-0.053769	3.898826
269.530701	5152.986484	16.027520	-0.053742	3.895927
269.606578	5145.022883	16.032525	-0.053751	3.893048
269.558402	5136.940470	16.037530	-0.053737	3.890123
269.411548	5128.982178	16.042535	-0.053705	3.887238
269.653509	5121.000139	16.047539	-0.053745	3.884350
269.369340	5113.022189	16.052544	-0.053687	3.881451
269.331880	5105.021903	16.057549	-0.053675	3.878547
269.153435	5097.010143	16.062554	-0.053636	3.875633
269.154659	5088.773486	16.067559	-0.053631	3.872639
269.042943	5080.821149	16.072563	-0.053605	3.869744
268.922762	5072.876982	16.077568	-0.053578	3.866850
269.078783	5064.919773	16.082573	-0.053602	3.863954
268.950355	5056.966611	16.087578	-0.053573	3.861052
268.779921	5048.978987	16.092583	-0.053536	3.858134
268.860201	5040.984791	16.097587	-0.053546	3.855216
268.735481	5032.975285	16.102592	-0.053518	3.852287
268.797225	5024.962635	16.107597	-0.053524	3.849358
268.802444	5016.977059	16.112602	-0.053520	3.846435
268.911543	5008.990157	16.117607	-0.053535	3.843512
268.731340	5001.046493	16.122611	-0.053497	3.840597
268.466335	4993.057476	16.127616	-0.053442	3.837661
268.599957	4985.017753	16.132621	-0.053462	3.834712
268.370419	4977.015398	16.137626	-0.053414	3.831768
268.473758	4969.012610	16.142631	-0.053428	3.828827
268.431272	4961.003740	16.147635	-0.053415	3.825879
268.365723	4953.042196	16.152640	-0.053398	3.822946
268.475511	4945.053200	16.157645	-0.053413	3.820004
268.265849	4937.105313	16.162650	-0.053369	3.817069
268.185188	4929.075145	16.167655	-0.053349	3.814103
268.201286	4921.049976	16.172659	-0.053347	3.811139
267.963455	4913.066670	16.177664	-0.053297	3.808183
268.063319	4905.068616	16.182669	-0.053311	3.805226
268.005536	4897.126273	16.187674	-0.053295	3.802284
268.080384	4889.097385	16.192679	-0.053304	3.799311
267.940703	4881.118323	16.197683	-0.053273	3.796349
268.030178	4873.027120	16.202688	-0.053284	3.793348
267.788701	4865.052339	16.207693	-0.053234	3.790381
267.423455	4857.065131	16.212698	-0.053161	3.787404
267.667867	4849.071217	16.217703	-0.053202	3.784436
267.680311	4841.079538	16.222707	-0.053199	3.781461
267.403025	4833.096201	16.227712	-0.053142	3.778480
267.569556	4825.100499	16.232717	-0.053168	3.775502
267.415905	4817.078244	16.237722	-0.053134	3.772505
267.381932	4809.099579	16.242727	-0.053123	3.769525
267.477449	4801.071063	16.247731	-0.053136	3.766526
267.411487	4793.115340	16.252736	-0.053118	3.763549
267.459373	4785.102398	16.257741	-0.053122	3.760550
267.382687	4777.119193	16.262746	-0.053103	3.757557
267.320703	4769.112367	16.267751	-0.053086	3.754554
267.159028	4761.092269	16.272755	-0.053051	3.751540
266.969379	4753.115301	16.277760	-0.053010	3.748540
267.087333	4745.091093	16.282765	-0.053027	3.745527
267.245106	4737.104863	16.287770	-0.053051	3.742526
267.191152	4729.131397	16.292775	-0.053036	3.739523
267.270359	4721.129626	16.297779	-0.053046	3.736510
267.068665	4713.121086	16.302784	-0.053003	3.733485
267.135406	4705.140464	16.307789	-0.053011	3.730475
266.886711	4697.176863	16.312794	-0.052959	3.727461
266.714345	4689.149818	16.317799	-0.052922	3.724423
266.833718	4681.191919	16.322803	-0.052939	3.721415
266.672341	4673.183918	16.327808	-0.052904	3.718380
266.852105	4665.179911	16.332813	-0.052932	3.715351
266.746403	4657.095952	16.337818	-0.052908	3.712283
266.492428	4649.076671	16.342823	-0.052855	3.709233
266.625375	4641.095281	16.347827	-0.052875	3.706204
266.402569	4633.152980	16.352832	-0.052828	3.703179
266.324950	4625.174326	16.357837	-0.052809	3.700141
266.339927	4617.177453	16.362842	-0.052806	3.697097
266.256590	4609.200887	16.367847	-0.052786	3.694054
266.313838	4601.207920	16.372851	-0.052791	3.691007
266.069952	4593.202677	16.377856	-0.052741	3.687945
266.267338	4585.171359	16.382861	-0.052772	3.684881
266.074593	4577.240690	16.387866	-0.052732	3.681844
266.127790	4569.245084	16.392871	-0.052736	3.678785
266.235996	4561.221534	16.397875	-0.052751	3.675715
266.162431	4553.184883	16.402880	-0.052733	3.672632
266.110871	4545.223515	16.407885	-0.052718	3.669576
265.950092	4537.202096	16.412890	-0.052683	3.666492
265.923524	4529.241100	16.417895	-0.052673	3.663432
265.969015	4521.238965	16.422899	-0.052676	3.660355
265.765611	4513.247229	16.427904	-0.052633	3.657273
265.586300	4505.258279	16.432909	-0.052595	3.654191
265.670243	4497.205834	16.437914	-0.052605	3.651088
265.637389	4489.236817	16.442919	-0.052594	3.648011
265.651795	4481.223678	16.447923	-0.052592	3.644917
265.522582	4473.262611	16.452928	-0.052562	3.641835
265.442895	4465.298521	16.457933	-0.052542	3.638752
265.356290	4457.290122	16.462938	-0.052521	3.635648
265.361399	4449.230796	16.467943	-0.052517	3.632525
265.550220	4441.236581	16.472947	-0.052547	3.629429
265.377609	4433.234616	16.477952	-0.052510	3.626317
265.338676	4425.280963	16.482957	-0.052498	3.623226
265.239808	4417.235567	16.487962	-0.052474	3.620094
265.286674	4409.289678	16.492967	-0.052478	3.617002
265.242022	4401.285653	16.497971	-0.052464	3.613883
265.043503	4393.268099	16.502976	-0.052422	3.610751
265.084482	4385.297594	16.507981	-0.052425	3.607641
264.934244	4377.288258	16.512986	-0.052392	3.604509
265.037800	4369.343116	16.517991	-0.052406	3.601406
265.041892	4361.357574	16.522995	-0.052402	3.598281
264.754349	4353.340659	16.528000	-0.052343	3.595133
264.727493	4345.372099	16.533005	-0.052333	3.592009
264.841222	4337.342410	16.538010	-0.052349	3.588862
264.707241	4329.336612	16.543015	-0.052319	3.585715
264.678409	4321.378817	16.548019	-0.052308	3.582587
264.600754	4313.365648	16.553024	-0.052289	3.579433
264.855268	4305.404631	16.558029	-0.052331	3.576306
264.589040	4297.390646	16.563034	-0.052276	3.573140
264.223488	4289.378418	16.568039	-0.052203	3.569970
264.364141	4281.411053	16.573043	-0.052224	3.566829
264.355408	4273.392012	16.578048	-0.052218	3.563660
264.251762	4265.439120	16.583053	-0.052193	3.560512
264.076926	4257.459101	16.588058	-0.052156	3.557349
264.092632	4249.388790	16.593063	-0.052153	3.554152
264.196231	4241.334225	16.598067	-0.052167	3.550961
264.240243	4233.335286	16.603072	-0.052171	3.547788
264.036911	4225.368063	16.608077	-0.052128	3.544618
264.001569	4217.421514	16.613082	-0.052116	3.541457
264.130198	4209.423624	16.618087	-0.052135	3.538278
264.244453	4201.415919	16.623091	-0.052151	3.535092
264.041458	4193.419521	16.628096	-0.052108	3.531899
263.872345	4185.413839	16.633101	-0.052072	3.528699
263.901484	4177.420144	16.638106	-0.052072	3.525507
263.940630	4169.471959	16.643111	-0.052074	3.522331
263.785076	4161.491812	16.648115	-0.052040	3.519134
263.459326	4153.507723	16.653120	-0.051974	3.515927
263.589418	4145.466117	16.658125	-0.051993	3.512707
263.530465	4137.453991	16.663130	-0.051977	3.509491
263.220955	4129.507985	16.668135	-0.051915	3.506291
263.529287	4121.492630	16.673139	-0.051967	3.503078
263.383861	4113.485927	16.678144	-0.051935	3.499853
263.305277	4105.558259	16.683149	-0.051915	3.496658
263.190499	4097.560146	16.688154	-0.051889	3.493431
263.197471	4089.485045	16.693159	-0.051885	3.490173
263.114026	4081.576728	16.698163	-0.051864	3.486977
263.245261	4073.545540	16.703168	-0.051883	3.483735
263.223230	4065.568414	16.708173	-0.051874	3.480508
262.937874	4057.607691	16.713178	-0.051816	3.477275
262.837949	4049.572249	16.718183	-0.051792	3.474015
262.922474	4041.563011	16.723187	-0.051803	3.470768
262.738760	4033.574637	16.728192	-0.051764	3.467519
262.728337	4025.589397	16.733197	-0.051757	3.464273
262.807600	4017.601496	16.738202	-0.051766	3.461026
262.782642	4009.607092	16.743207	-0.051756	3.457769
262.512049	4001.642801	16.748211	-0.051701	3.454514
262.436588	3993.586482	16.753216	-0.051682	3.451225
262.491875	3985.592401	16.758221	-0.051687	3.447962
262.483913	3977.622377	16.763226	-0.051680	3.444704
262.260194	3969.648982	16.768231	-0.051634	3.441434
262.503015	3961.683111	16.773235	-0.051674	3.438180
262.280153	3953.659428	16.778240	-0.051627	3.434884
262.428824	3945.624197	16.783245	-0.051650	3.431591
262.324435	3937.629256	16.788250	-0.051625	3.428304
262.302854	3929.650497	16.793255	-0.051616	3.425023
262.194953	3921.723577	16.798259	-0.051591	3.421758
261.929853	3913.731492	16.803264	-0.051537	3.418457
262.227908	3905.703495	16.808269	-0.051587	3.415157
262.186468	3897.695059	16.813274	-0.051574	3.411850
261.919015	3889.701643	16.818279	-0.051519	3.408539
261.907998	3881.721426	16.823283	-0.051512	3.405239
261.824148	3873.779090	16.828288	-0.051491	3.401949
261.796017	3865.785644	16.833293	-0.051481	3.398636
261.841694	3857.797654	16.838298	-0.051484	3.395325
261.877545	3849.675434	16.843303	-0.051486	3.391954
261.736426	3841.710435	16.848307	-0.051455	3.388640
261.302811	3833.743213	16.853312	-0.051369	3.385311
261.370592	3825.779547	16.858317	-0.051376	3.381997
261.422361	3817.780079	16.863322	-0.051381	3.378665
261.358532	3809.791469	16.868327	-0.051364	3.375330
261.530002	3801.791707	16.873331	-0.051391	3.371995
261.338836	3793.784130	16.878336	-0.051350	3.368642
261.367857	3785.816692	16.883341	-0.051350	3.365309
261.116561	3777.855594	16.888346	-0.051298	3.361965
261.171218	3769.846746	16.893351	-0.051303	3.358610
261.224928	3761.861576	16.898355	-0.051308	3.355260
261.364416	3753.830233	16.903360	-0.051329	3.351891
261.226796	3745.853636	16.908365	-0.051299	3.348532
261.186211	3737.825637	16.913370	-0.051286	3.345151
260.952261	3729.908313	16.918375	-0.051237	3.341807
261.043757	3721.905869	16.923379	-0.051249	3.338435
261.014233	3713.906409	16.928384	-0.051239	3.335056
260.933367	3705.889989	16.933389	-0.051218	3.331665
260.715899	3697.919446	16.938394	-0.051173	3.328285
260.676242	3689.910692	16.943399	-0.051160	3.324891
260.615622	3681.985569	16.948403	-0.051144	3.321529
260.565236	3673.988198	16.953408	-0.051130	3.318133
260.418890	3665.997163	16.958413	-0.051097	3.314733
260.699173	3657.934394	16.963418	-0.051144	3.311315
260.600084	3649.944715	16.968423	-0.051121	3.307910
260.459921	3641.961077	16.973427	-0.051089	3.304503
260.387982	3633.961429	16.978432	-0.051071	3.301088
260.324175	3626.040989	16.983437	-0.051054	3.297703
260.291552	3618.036160	16.988442	-0.051043	3.294280
260.344163	3610.005837	16.993447	-0.051048	3.290846
260.337874	3602.051773	16.998451	-0.051041	3.287439
260.138379	3594.051181	17.003456	-0.050999	3.284000
259.989160	3586.102545	17.008461	-0.050966	3.280583
260.187387	3578.107853	17.013466	-0.050998	3.277155
260.086544	3570.072885	17.018471	-0.050974	3.273695
259.885359	3562.091014	17.023475	-0.050932	3.270250
259.979740	3554.080103	17.028480	-0.050944	3.266801
260.004924	3546.093998	17.033485	-0.050944	3.263355
259.730607	3538.130481	17.038490	-0.050887	3.259905
259.627766	3530.172213	17.043495	-0.050863	3.256459
259.712593	3522.159194	17.048499	-0.050874	3.252994
259.634165	3514.127097	17.053504	-0.050854	3.249510
259.558101	3506.183278	17.058509	-0.050835	3.246061
259.553920	3498.211176	17.063514	-0.050829	3.242598
259.496298	3490.192932	17.068519	-0.050813	3.239110
259.522643	3482.241587	17.073523	-0.050813	3.235651
259.322447	3474.164226	17.078528	-0.050771	3.232124
259.301882	3466.165023	17.083533	-0.050762	3.228634
259.341784	3458.165306	17.088538	-0.050764	3.225142
259.128921	3450.241250	17.093543	-0.050719	3.221670
259.255658	3442.245044	17.098547	-0.050738	3.218176
259.043971	3434.239869	17.103552	-0.050693	3.214661
259.082221	3426.247954	17.108557	-0.050695	3.211158
259.080240	3418.283437	17.113562	-0.050690	3.207661
258.778496	3410.311716	17.118567	-0.050629	3.204145
258.899958	3402.333220	17.123571	-0.050646	3.200640
258.936273	3394.340261	17.128576	-0.050648	3.197121
259.032622	3386.313623	17.133581	-0.050661	3.193585
258.796369	3378.343552	17.138586	-0.050612	3.190057
258.635547	3370.349143	17.143591	-0.050577	3.186517
258.755637	3362.380742	17.148595	-0.050594	3.182997
258.612808	3354.372860	17.153600	-0.050562	3.179444
258.605348	3346.416683	17.158605	-0.050556	3.175916
258.577394	3338.410161	17.163610	-0.050545	3.172361
258.573558	3330.399087	17.168615	-0.050539	3.168800
258.577623	3322.413796	17.173619	-0.050535	3.165248
258.156632	3314.469938	17.178624	-0.050452	3.161691
258.372125	3306.459907	17.183629	-0.050487	3.158129
258.221593	3298.482268	17.188634	-0.050454	3.154561
258.158279	3290.458517	17.193639	-0.050437	3.150972
258.261107	3282.466889	17.198643	-0.050451	3.147401
258.261830	3274.478179	17.203648	-0.050446	3.143823
258.152096	3266.505839	17.208653	-0.050420	3.140243
258.061808	3258.561601	17.213658	-0.050398	3.136672
257.889751	3250.551146	17.218663	-0.050361	3.133064
257.879332	3242.564689	17.223667	-0.050354	3.129470
257.757271	3234.551274	17.228672	-0.050326	3.125854
257.756237	3226.607933	17.233677	-0.050321	3.122271
257.778649	3218.620271	17.238682	-0.050320	3.118665
257.534379	3210.650214	17.243687	-0.050270	3.115051
257.643289	3202.620138	17.248691	-0.050285	3.111422
257.467301	3194.632428	17.253696	-0.050247	3.107794
257.394525	3186.639762	17.258701	-0.050228	3.104165
257.326951	3178.658027	17.263706	-0.050211	3.100536
257.311115	3170.707274	17.268711	-0.050203	3.096920
257.534024	3162.681667	17.273715	-0.050239	3.093276
257.443284	3154.657086	17.278720	-0.050217	3.089615
257.218405	3146.723202	17.283725	-0.050170	3.085984
257.173993	3138.762889	17.288730	-0.050157	3.082345
256.977460	3130.776835	17.293735	-0.050115	3.078683
257.256160	3122.799475	17.298739	-0.050162	3.075042
257.159151	3114.694497	17.303744	-0.050139	3.071321
256.859750	3106.749694	17.308749	-0.050078	3.067660
256.865417	3098.778159	17.313754	-0.050074	3.063996
256.922136	3090.771645	17.318759	-0.050079	3.060315
257.021188	3082.840858	17.323763	-0.050093	3.056665
256.771314	3074.832659	17.328768	-0.050041	3.052960
256.813591	3066.835531	17.333773	-0.050044	3.049268
256.796710	3058.876393	17.338778	-0.050035	3.045587
256.436006	3050.923745	17.343783	-0.049963	3.041888
256.868476	3042.912896	17.348787	-0.050039	3.038195
256.567758	3034.925217	17.353792	-0.049978	3.034474
256.550445	3026.924969	17.358797	-0.049969	3.030756
256.464004	3018.951754	17.363802	-0.049948	3.027042
256.408384	3010.960396	17.368807	-0.049933	3.023317
256.328582	3003.014206	17.373811	-0.049913	3.019607
256.239834	2995.033988	17.378816	-0.049891	3.015876
256.356391	2987.012282	17.383821	-0.049908	3.012131
256.153351	2979.043836	17.388826	-0.049865	3.008391
256.033122	2971.046130	17.393831	-0.049837	3.004637
256.004973	2963.102692	17.398835	-0.049827	3.000907
256.194178	2955.088571	17.403840	-0.049857	2.997151
256.035009	2947.108420	17.408845	-0.049822	2.993389
255.978010	2939.099146	17.413850	-0.049807	2.989613
255.933824	2931.111900	17.418855	-0.049793	2.985843
255.853241	2923.164378	17.423859	-0.049773	2.982086
255.753186	2915.166295	17.428864	-0.049749	2.978299
255.588828	2907.208983	17.433869	-0.049714	2.974523
255.646367	2899.192866	17.438874	-0.049719	2.970726
255.554199	2891.216713	17.443879	-0.049697	2.966935
255.540563	2883.243740	17.448883	-0.049690	2.963145
255.539657	2875.263880	17.453888	-0.049684	2.959348
255.412935	2867.324760	17.458893	-0.049656	2.955558
255.296070	2859.294129	17.463898	-0.049629	2.951721
255.256638	2851.295724	17.468903	-0.049616	2.947897
255.348657	2843.323569	17.473907	-0.049628	2.944088
255.051396	2835.358720	17.478912	-0.049568	2.940258
255.212771	2827.376325	17.483917	-0.049593	2.936438
255.062413	2819.393795	17.488922	-0.049560	2.932597
254.923054	2811.375195	17.493927	-0.049529	2.928734
254.864986	2803.439415	17.498931	-0.049513	2.924909
254.714041	2795.467205	17.503936	-0.049480	2.921058
254.774657	2787.499978	17.508941	-0.049486	2.917215
254.761263	2779.465463	17.513946	-0.049478	2.913330
254.724278	2771.404293	17.518951	-0.049466	2.909426
254.860126	2763.439938	17.523955	-0.049486	2.905573
254.670589	2755.490945	17.528960	-0.049446	2.901704
254.787330	2747.513832	17.533965	-0.049463	2.897834
254.787939	2739.542801	17.538970	-0.049458	2.893955
254.570304	2731.545084	17.543975	-0.049412	2.890046
254.733036	2723.571872	17.548979	-0.049437	2.886164
254.580503	2715.619319	17.553984	-0.049404	2.882270
254.620708	2707.653021	17.558989	-0.049406	2.878374
254.377323	2699.714362	17.563994	-0.049356	2.874471
254.422778	2691.647625	17.568999	-0.049359	2.870516
254.476092	2683.685723	17.574003	-0.049364	2.866607
254.145024	2675.738917	17.579008	-0.049297	2.862679
253.997945	2667.769937	17.584013	-0.049265	2.858745
254.148089	2659.778048	17.589018	-0.049288	2.854811
253.975068	2651.773398	17.594023	-0.049250	2.850847
254.003598	2643.819101	17.599027	-0.049251	2.846914
253.930745	2635.826120	17.604032	-0.049232	2.842950
253.839967	2627.872133	17.609037	-0.049210	2.838999
253.674080	2619.917667	17.614042	-0.049174	2.835038
253.729660	2611.862146	17.619047	-0.049179	2.831034
253.689018	2603.902807	17.624051	-0.049167	2.827066
253.604447	2595.919634	17.629056	-0.049146	2.823079
253.486281	2587.975965	17.634061	-0.049119	2.819104
253.426254	2580.001389	17.639066	-0.049102	2.815111
253.444921	2571.975616	17.644071	-0.049101	2.811091
253.308483	2564.028188	17.649075	-0.049070	2.807096
253.219713	2556.054396	17.654080	-0.049049	2.803084
253.327818	2548.074415	17.659085	-0.049064	2.799075
253.185672	2540.125928	17.664090	-0.049032	2.795062
253.100355	2532.108815	17.669095	-0.049011	2.791011
253.350114	2524.106687	17.674099	-0.049053	2.786982
253.070543	2516.162402	17.679104	-0.048995	2.782945
252.916942	2508.193048	17.684109	-0.048962	2.778897
253.002708	2500.218683	17.689114	-0.048973	2.774855
252.796255	2492.222336	17.694119	-0.048929	2.770778
252.868054	2484.263702	17.699123	-0.048937	2.766731
252.764088	2476.297389	17.704128	-0.048913	2.762664
252.878543	2468.314910	17.709133	-0.048929	2.758595
252.859461	2460.333528	17.714138	-0.048921	2.754513
252.767422	2452.245815	17.719143	-0.048898	2.750366
252.648807	2444.318248	17.724147	-0.048871	2.746294
252.676160	2436.363478	17.729152	-0.048871	2.742210
252.564606	2428.409606	17.734157	-0.048845	2.738112
252.628958	2420.437868	17.739162	-0.048852	2.734009
252.392845	2412.427696	17.744167	-0.048803	2.729862
252.176821	2404.501108	17.749171	-0.048758	2.725753
252.361797	2396.497459	17.754176	-0.048787	2.721623
252.414070	2388.533650	17.759181	-0.048792	2.717499
252.166998	2380.585646	17.764186	-0.048741	2.713358
252.099768	2372.565480	17.769191	-0.048723	2.709185
252.249722	2364.582722	17.774195	-0.048746	2.705038
252.324224	2356.615153	17.779200	-0.048755	2.700888
252.072487	2348.697645	17.784205	-0.048703	2.696737
251.968285	2340.709174	17.789210	-0.048678	2.692552
251.920293	2332.709161	17.794215	-0.048664	2.688358
251.924503	2324.756995	17.799219	-0.048660	2.684185
251.739519	2316.787153	17.804224	-0.048620	2.679985
251.564231	2308.861335	17.809229	-0.048583	2.675803
251.627392	2300.825691	17.814234	-0.048589	2.671570
251.434239	2292.854451	17.819239	-0.048548	2.667349
251.559321	2284.874453	17.824243	-0.048567	2.663137
251.449000	2276.912629	17.829248	-0.048541	2.658913
251.466102	2268.945077	17.834253	-0.048539	2.654687
251.490293	2260.950590	17.839258	-0.048538	2.650440
251.335346	2252.976694	17.844263	-0.048505	2.646186
251.246357	2245.050654	17.849267	-0.048483	2.641955
251.209039	2237.069690	17.854272	-0.048471	2.637691
251.363190	2229.070588	17.859277	-0.048494	2.633423
251.320439	2221.092529	17.864282	-0.048481	2.629147
251.117615	2213.129722	17.869287	-0.048439	2.624861
251.156966	2205.182702	17.874291	-0.048441	2.620592
250.956872	2197.233241	17.879296	-0.048398	2.616300
250.806359	2189.242796	17.884301	-0.048365	2.611981
250.819133	2181.261608	17.889306	-0.048363	2.607671
250.888481	2173.269579	17.894311	-0.048370	2.603352
250.861889	2165.323116	17.899315	-0.048360	2.599045
250.614079	2157.383735	17.904320	-0.048309	2.594718
250.577825	2149.203620	17.909325	-0.048297	2.590268
250.728878	2141.251318	17.914330	-0.048320	2.585947
250.626091	2133.322778	17.919335	-0.048296	2.581615
250.699840	2125.390647	17.924339	-0.048305	2.577285
250.522195	2117.449741	17.929344	-0.048267	2.572926
250.320715	2109.492106	17.934349	-0.048224	2.568549
250.363389	2101.531368	17.939354	-0.048227	2.564180
250.352345	2093.573641	17.944359	-0.048220	2.559801
250.433791	2085.628338	17.949363	-0.048230	2.555427
250.127501	2077.653183	17.954368	-0.048168	2.551003
249.996076	2069.687970	17.959373	-0.048138	2.546589
250.139967	2061.708515	17.964378	-0.048160	2.542178
249.968095	2053.757311	17.969383	-0.048123	2.537753
250.026367	2045.793630	17.974387	-0.048129	2.533330
249.835763	2037.820047	17.979392	-0.048088	2.528876
249.729215	2029.858294	17.984397	-0.048063	2.524426
249.741264	2021.904703	17.989402	-0.048060	2.519982
249.625967	2013.957180	17.994407	-0.048034	2.515524
249.434819	2005.967066	17.999411	-0.047993	2.511029
249.409154	1997.980140	18.004416	-0.047983	2.506539
249.436385	1990.015422	18.009421	-0.047983	2.502058
249.420167	1982.061413	18.014426	-0.047975	2.497571
249.374837	1974.079072	18.019431	-0.047962	2.493059
249.434749	1966.103411	18.024435	-0.047968	2.488549
249.148639	1958.171201	18.029440	-0.047909	2.484031
248.960820	1950.240324	18.034445	-0.047869	2.479512
249.176044	1942.254781	18.039450	-0.047904	2.474984
249.227023	1934.241292	18.044455	-0.047909	2.470419
249.155122	1926.298416	18.049459	-0.047890	2.465878
248.880026	1918.377862	18.054464	-0.047834	2.461325
248.925568	1910.398490	18.059469	-0.047837	2.456754
248.889966	1902.443713	18.064474	-0.047826	2.452183
248.666351	1894.485552	18.069479	-0.047779	2.447587
248.615520	1886.533097	18.074483	-0.047764	2.442998
248.575515	1878.578796	18.079488	-0.047752	2.438401
248.481741	1870.597529	18.084493	-0.047729	2.433775
248.495633	1862.566485	18.089498	-0.047727	2.429120
248.610604	1854.571328	18.094503	-0.047743	2.424484
248.702703	1846.635931	18.099507	-0.047755	2.419873
248.574821	1838.698929	18.104512	-0.047726	2.415235
248.312298	1830.756627	18.109517	-0.047672	2.410574
248.440439	1822.808440	18.114522	-0.047691	2.405932
248.230097	1814.868049	18.119527	-0.047647	2.401258
248.176541	1806.930629	18.124531	-0.047632	2.396590
248.056331	1798.957453	18.129536	-0.047604	2.391885
248.071432	1790.962697	18.134541	-0.047602	2.387170
247.926557	1783.030401	18.139546	-0.047570	2.382469
247.884680	1775.064530	18.144551	-0.047557	2.377748
248.097018	1767.095178	18.149555	-0.047592	2.373035
247.849890	1759.148307	18.154560	-0.047541	2.368290
247.638223	1751.204381	18.159565	-0.047496	2.363539
247.827378	1743.241722	18.164570	-0.047526	2.358800
247.565139	1735.300719	18.169575	-0.047472	2.354028
247.570793	1727.318003	18.174579	-0.047468	2.349243
247.542892	1719.341272	18.179584	-0.047458	2.344449
247.746498	1711.374165	18.184589	-0.047491	2.339670
247.468809	1703.475967	18.189594	-0.047434	2.334883
247.287985	1695.485027	18.194599	-0.047395	2.330039
247.493179	1687.520947	18.199603	-0.047428	2.325232
247.224095	1679.611749	18.204608	-0.047373	2.320409
247.200478	1671.675983	18.209613	-0.047364	2.315581
247.327792	1663.687317	18.214618	-0.047382	2.310722
247.076447	1655.732614	18.219623	-0.047331	2.305843
247.068057	1647.802434	18.224627	-0.047324	2.300989
246.996562	1639.848307	18.229632	-0.047306	2.296104
246.992998	1631.879244	18.234637	-0.047300	2.291205
246.713647	1623.969404	18.239642	-0.047243	2.286309
246.644603	1616.010874	18.244647	-0.047225	2.281391
246.753161	1608.051374	18.249651	-0.047240	2.276476
246.548236	1600.045336	18.254656	-0.047197	2.271495
246.367031	1592.096120	18.259661	-0.047158	2.266540
246.690319	1584.119141	18.264666	-0.047213	2.261601
246.477728	1576.214855	18.269671	-0.047168	2.256649
246.610581	1568.230264	18.274675	-0.047188	2.251667
246.512817	1560.281349	18.279680	-0.047165	2.246676
246.345668	1552.372959	18.284685	-0.047129	2.241693
246.242349	1544.468904	18.289690	-0.047104	2.236707
246.031150	1536.503935	18.294695	-0.047060	2.231662
246.180955	1528.518755	18.299699	-0.047083	2.226625
245.960050	1520.594777	18.304704	-0.047037	2.221583
245.839863	1512.667213	18.309709	-0.047009	2.216535
245.912546	1504.695462	18.314714	-0.047018	2.211465
245.832407	1496.740674	18.319719	-0.046998	2.206381
245.814220	1488.817971	18.324723	-0.046989	2.201310
245.633003	1480.894661	18.329728	-0.046950	2.196213
245.709182	1472.897026	18.334733	-0.046959	2.191080
245.581772	1464.967391	18.339738	-0.046931	2.185960
245.451912	1457.026817	18.344743	-0.046901	2.180821
245.416579	1449.107546	18.349747	-0.046890	2.175691
245.488884	1441.131374	18.354752	-0.046898	2.170523
245.363718	1433.189470	18.359757	-0.046870	2.165347
245.422674	1425.269862	18.364762	-0.046876	2.160189
245.252920	1417.342269	18.369767	-0.046839	2.154993
245.145843	1409.404258	18.374771	-0.046814	2.149783
245.176872	1401.432112	18.379776	-0.046815	2.144551
245.057742	1393.517195	18.384781	-0.046787	2.139330
244.996220	1385.595227	18.389786	-0.046771	2.134097
244.818513	1377.634428	18.394791	-0.046733	2.128814
244.987990	1369.687618	18.399795	-0.046759	2.123560
244.641719	1361.818062	18.404800	-0.046690	2.118295
244.660446	1353.835054	18.409805	-0.046688	2.112977
244.758477	1345.836879	18.414810	-0.046701	2.107642
244.621063	1337.906111	18.419815	-0.046671	2.102317
244.612437	1329.991299	18.424819	-0.046664	2.097001
244.482282	1322.059946	18.429824	-0.046635	2.091649
244.454235	1314.117311	18.434829	-0.046624	2.086285
244.522945	1306.195574	18.439834	-0.046632	2.080931
244.386193	1298.285174	18.444839	-0.046602	2.075551
244.551862	1290.311254	18.449843	-0.046627	2.070143
244.402468	1282.389983	18.454848	-0.046595	2.064726
244.140979	1274.511646	18.459853	-0.046541	2.059313
244.080982	1266.588158	18.464858	-0.046525	2.053874
244.063805	1258.616372	18.469863	-0.046516	2.048393
243.967345	1250.713714	18.474867	-0.046493	2.042936
243.813819	1242.812848	18.479872	-0.046460	2.037460
243.805272	1234.845440	18.484877	-0.046453	2.031938
243.846220	1226.898676	18.489882	-0.046456	2.026420
243.579168	1218.992900	18.494887	-0.046401	2.020884
243.672028	1211.064829	18.499891	-0.046413	2.015354
243.653754	1203.122095	18.504896	-0.046405	2.009787
243.406424	1195.217910	18.509901	-0.046354	2.004209
243.487018	1187.306170	18.514906	-0.046363	1.998643
243.452035	1179.369301	18.519911	-0.046352	1.993032
243.316066	1171.444909	18.524915	-0.046322	1.987403
243.183897	1163.535025	18.529920	-0.046292	1.981769
243.354997	1155.596244	18.534925	-0.046319	1.976131
243.374954	1147.658626	18.539930	-0.046317	1.970461
243.122781	1139.760916	18.544935	-0.046265	1.964774
242.952777	1131.889805	18.549939	-0.046229	1.959099
243.063590	1123.922412	18.554944	-0.046244	1.953368
242.876813	1115.978217	18.559949	-0.046204	1.947604
242.769889	1108.086099	18.564954	-0.046179	1.941870
242.739932	1100.150497	18.569959	-0.046169	1.936096
242.578606	1092.255107	18.574963	-0.046134	1.930319
242.511187	1084.333739	18.579968	-0.046116	1.924517
242.676875	1076.399239	18.584973	-0.046142	1.918713
242.740897	1068.477026	18.589978	-0.046149	1.912889
242.479522	1060.573346	18.594983	-0.046095	1.907024
242.542899	1052.663129	18.599987	-0.046102	1.901173
242.653422	1044.748422	18.604992	-0.046117	1.895306
242.277272	1036.875025	18.609997	-0.046042	1.889397
242.123390	1028.993624	18.615002	-0.046009	1.883488
242.046324	1021.088999	18.620007	-0.045989	1.877552
241.990274	1013.168081	18.625011	-0.045974	1.871587
241.939212	1005.236765	18.630016	-0.045959	1.865596
241.750486	997.355448	18.635021	-0.045919	1.859607
241.877501	989.437023	18.640026	-0.045938	1.853608
241.809869	981.509245	18.645031	-0.045920	1.847559
241.732969	973.632109	18.650035	-0.045901	1.841528
241.686762	965.743386	18.655040	-0.045887	1.835471
241.529806	957.834329	18.660045	-0.045853	1.829366
241.619694	949.917238	18.665050	-0.045864	1.823264
241.581083	942.021377	18.670055	-0.045852	1.817142
241.460458	934.144114	18.675059	-0.045825	1.811004
241.309437	926.253764	18.680064	-0.045792	1.804832
241.134165	918.390864	18.685069	-0.045754	1.798656
241.360823	910.431766	18.690074	-0.045791	1.792433
241.003604	902.538931	18.695079	-0.045719	1.786169
240.971035	894.660739	18.700083	-0.045708	1.779934
240.951273	886.768878	18.705088	-0.045700	1.773668
240.932889	878.857318	18.710093	-0.045691	1.767364
240.751692	871.018024	18.715098	-0.045652	1.761075
240.708239	863.128271	18.720103	-0.045639	1.754741
240.658064	855.227988	18.725107	-0.045625	1.748374
240.593070	847.347421	18.730112	-0.045608	1.741997
240.728766	839.441257	18.735117	-0.045628	1.735602
240.480805	831.597560	18.740122	-0.045577	1.729186
240.368499	823.716499	18.745127	-0.045551	1.722732
240.471377	815.837875	18.750131	-0.045565	1.716284
240.503202	807.930044	18.755136	-0.045566	1.709778
240.211871	800.082183	18.760141	-0.045507	1.703254
240.269126	792.214546	18.765146	-0.045512	1.696735
240.225106	784.322113	18.770151	-0.045499	1.690157
240.036181	776.482735	18.775155	-0.045459	1.683578
239.914912	768.632240	18.780160	-0.045431	1.676973
239.721977	760.755868	18.785165	-0.045390	1.670310
239.955654	752.857570	18.790170	-0.045429	1.663660
239.873843	744.998840	18.795175	-0.045409	1.656973
239.741542	737.141519	18.800179	-0.045379	1.650254
239.534377	729.311270	18.805184	-0.045335	1.643521
239.449548	721.468942	18.810189	-0.045315	1.636766
239.405112	713.553339	18.815194	-0.045301	1.629925
239.329239	705.674709	18.820199	-0.045282	1.623083
239.330265	697.823988	18.825203	-0.045277	1.616247
239.202452	689.979658	18.830208	-0.045249	1.609370
239.028327	682.148147	18.835213	-0.045211	1.602468
239.224867	674.276333	18.840218	-0.045243	1.595553
238.952866	666.437000	18.845223	-0.045187	1.588570
238.865021	658.603075	18.850227	-0.045166	1.581587
238.996427	650.740213	18.855232	-0.045185	1.574579
239.042128	642.879980	18.860237	-0.045189	1.567529
238.936378	635.071834	18.865242	-0.045164	1.560473
238.730580	627.255213	18.870247	-0.045121	1.553362
238.632823	619.401426	18.875251	-0.045097	1.546201
238.556941	611.577610	18.880256	-0.045078	1.539036
238.535703	603.740839	18.885261	-0.045069	1.531835
238.369767	595.935000	18.890266	-0.045034	1.524606
238.144225	588.138023	18.895271	-0.044987	1.517342
238.078755	580.296168	18.900275	-0.044969	1.510026
238.210409	572.452022	18.905280	-0.044989	1.502701
237.993396	564.658418	18.910285	-0.044944	1.495335
237.943257	556.845316	18.915290	-0.044929	1.487940
237.905138	549.025793	18.920295	-0.044917	1.480504
237.811815	541.222427	18.925299	-0.044895	1.473036
237.740101	533.368322	18.930304	-0.044876	1.465486
237.660077	525.575243	18.935309	-0.044857	1.457954
237.736712	517.754465	18.940314	-0.044866	1.450380
237.459211	509.989644	18.945319	-0.044809	1.442765
237.310435	502.213719	18.950323	-0.044777	1.435119
237.324982	494.399766	18.955328	-0.044774	1.427422
237.140559	486.628940	18.960333	-0.044735	1.419692
237.121136	478.842025	18.965338	-0.044726	1.411932
237.092398	471.044511	18.970343	-0.044716	1.404116
237.042900	463.287739	18.975347	-0.044702	1.396294
236.934492	455.497938	18.980352	-0.044677	1.388385
236.743237	447.740171	18.985357	-0.044636	1.380449
236.911953	439.943601	18.990362	-0.044663	1.372489
236.643731	432.199838	18.995367	-0.044608	1.364462
236.559225	424.452496	19.000371	-0.044587	1.356415
236.451982	416.689089	19.005376	-0.044562	1.348299
236.433359	408.920847	19.010381	-0.044554	1.340145
236.346725	401.190128	19.015386	-0.044533	1.331968
236.104361	393.468895	19.020391	-0.044483	1.323723
236.088233	385.728715	19.025395	-0.044475	1.315447
235.960719	377.866085	19.030400	-0.044446	1.306966
235.984732	370.124482	19.035405	-0.044445	1.298589
236.130366	362.380775	19.040410	-0.044468	1.290177
235.913533	354.692875	19.045415	-0.044422	1.281705
235.822359	347.001672	19.050419	-0.044401	1.273195
235.589867	339.311719	19.055424	-0.044352	1.264603
235.506214	331.612574	19.060429	-0.044332	1.255971
235.391403	323.922914	19.065434	-0.044306	1.247283
235.258451	316.244518	19.070439	-0.044276	1.238544
235.290305	308.523063	19.075443	-0.044277	1.229725
235.486248	300.791686	19.080448	-0.044308	1.220863
235.127576	293.171747	19.085453	-0.044237	1.211956
235.051295	285.506861	19.090458	-0.044218	1.202987
235.112534	277.825826	19.095463	-0.044224	1.193959
234.830115	270.201055	19.100467	-0.044167	1.184860
234.616591	262.578330	19.105472	-0.044122	1.175706
234.416510	254.939860	19.110477	-0.044080	1.166464
234.583605	247.284404	19.115482	-0.044106	1.157205
234.228368	239.648609	19.120487	-0.044035	1.147784
234.367062	231.993768	19.125491	-0.044056	1.138367
234.216183	224.384639	19.130496	-0.044023	1.128867
234.162316	216.775402	19.135501	-0.044008	1.119307
234.271424	209.152998	19.140506	-0.044024	1.109683
234.160017	201.568670	19.145511	-0.043998	1.099975
233.898599	194.029323	19.150515	-0.043945	1.090206
233.847095	186.456212	19.155520	-0.043930	1.080351
233.337147	178.958078	19.160525	-0.043831	1.070400
233.361673	171.384127	19.165530	-0.043830	1.060377
233.162321	163.851656	19.170535	-0.043788	1.050262
233.206124	156.301866	19.175539	-0.043792	1.040083
233.180483	148.772035	19.180544	-0.043782	1.029814
232.948676	141.283149	19.185549	-0.043734	1.019448
232.951607	133.778832	19.190554	-0.043730	1.009011
232.769770	126.317020	19.195559	-0.043691	0.998480
232.560479	118.839806	19.200563	-0.043648	0.987808
232.196698	111.422009	19.205568	-0.043575	0.977065
231.916680	103.994452	19.210573	-0.043518	0.966211
231.880457	96.561497	19.215578	-0.043507	0.955287
231.002639	89.263236	19.220583	-0.043339	0.944219
230.685857	81.890629	19.225587	-0.043275	0.933055
230.354529	74.534375	19.230592	-0.043209	0.921777
229.658011	67.248933	19.235597	-0.043074	0.910369
229.316293	60.144479	19.240602	-0.043006	0.899198