Tue Mar 23 11:23:51 2021

Number of Points = 3622
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
1.245633	-0.173802	0.000000	-0.000018	0.722401

1.180779	-0.172507	0.005005	-0.000006	0.722381
1.375650	-0.202547	0.010010	-0.000042	0.722390
1.207262	-0.179244	0.015014	-0.000011	0.722377
1.408161	-0.213735	0.020019	-0.000048	0.722380
1.186660	-0.172314	0.025024	-0.000007	0.722384
1.470679	-0.226013	0.030029	-0.000060	0.722378
1.517428	-0.230001	0.035034	-0.000069	0.722387
1.454693	-0.222169	0.040038	-0.000057	0.722380
1.338474	-0.200404	0.045043	-0.000036	0.722383
1.359676	-0.203263	0.050048	-0.000040	0.722384
1.327667	-0.200702	0.055053	-0.000034	0.722378
1.351323	-0.200182	0.060058	-0.000038	0.722388
1.338780	-0.202517	0.065062	-0.000036	0.722379
1.263323	-0.292269	0.070067	-0.000022	0.722177
1.173357	-0.315102	0.075072	-0.000005	0.722100
1.243381	-0.333286	0.080077	-0.000018	0.722089
1.380305	-0.354045	0.085082	-0.000044	0.722097
1.305048	-0.346683	0.090086	-0.000030	0.722085
1.272429	-0.339166	0.095091	-0.000024	0.722088
1.366448	-0.366071	0.100096	-0.000042	0.722069
1.319923	-0.515606	0.105101	-0.000033	0.721759
1.333790	-0.516603	0.110106	-0.000036	0.721762
1.290867	-0.513367	0.115110	-0.000028	0.721753
1.462432	-0.541804	0.120115	-0.000060	0.721757
1.319134	-0.535984	0.125120	-0.000033	0.721719
1.260245	-0.663557	0.130125	-0.000022	0.721448
1.495437	-0.701339	0.135130	-0.000066	0.721456
1.383149	-0.685751	0.140134	-0.000045	0.721447
1.178581	-0.648456	0.145139	-0.000007	0.721449
1.189026	-0.802166	0.150144	-0.000009	0.721151
1.081757	-0.794372	0.155149	0.000011	0.721128
1.186862	-0.810147	0.160154	-0.000009	0.721134
1.210327	-0.833563	0.165158	-0.000013	0.721097
1.329498	-0.963690	0.170163	-0.000036	0.720883
1.563383	-1.003505	0.175168	-0.000079	0.720886
1.305150	-0.959352	0.180173	-0.000031	0.720883
1.365480	-1.110488	0.185178	-0.000042	0.720607
1.175312	-1.108022	0.190182	-0.000007	0.720545
1.346686	-1.137066	0.195187	-0.000039	0.720548
1.471102	-1.280845	0.200192	-0.000062	0.720309
1.272858	-1.286793	0.205197	-0.000025	0.720228
1.141482	-1.259002	0.210202	-0.000001	0.720236
1.127153	-1.406145	0.215206	0.000002	0.719942
1.124683	-1.424277	0.220211	0.000002	0.719905
1.024328	-1.419554	0.225216	0.000021	0.719879
1.186829	-1.588370	0.230221	-0.000010	0.719604
0.943340	-1.540976	0.235226	0.000036	0.719612
0.573942	-1.547635	0.240230	0.000104	0.719469
0.594117	-1.648060	0.245235	0.000101	0.719278
0.636539	-1.652605	0.250240	0.000093	0.719284
0.480629	-1.743051	0.255245	0.000122	0.719051
0.488899	-1.782532	0.260250	0.000120	0.718977
0.357088	-1.779071	0.265254	0.000144	0.718937
0.369382	-1.924159	0.270259	0.000142	0.718655
0.442883	-1.937166	0.275264	0.000128	0.718656
0.371675	-2.018285	0.280269	0.000142	0.718471
0.601465	-2.110736	0.285274	0.000099	0.718369
0.412198	-2.123461	0.290278	0.000134	0.718277
0.213226	-2.213418	0.295283	0.000171	0.718030
0.028892	-2.178774	0.300288	0.000205	0.718034
-0.905069	-2.160660	0.305293	0.000379	0.717741
-1.690991	-2.031676	0.310298	0.000525	0.717719
-2.033131	-1.974378	0.315302	0.000589	0.717712
-1.458034	-2.225281	0.320307	0.000482	0.717419
-2.314548	-2.085849	0.325312	0.000641	0.717393
-1.992386	-2.147600	0.330317	0.000581	0.717384
-2.639781	-2.166566	0.335322	0.000702	0.717119
-3.408176	-2.043606	0.340326	0.000845	0.717092
-2.955317	-2.125003	0.345331	0.000760	0.717090
-3.116947	-2.174386	0.350336	0.000790	0.716936
-4.624232	-1.994469	0.355341	0.001071	0.716761
-3.934526	-2.111859	0.360346	0.000942	0.716772
-4.111362	-2.084307	0.365350	0.000975	0.716764
-4.574541	-2.079592	0.370355	0.001061	0.716610
-5.111582	-2.057527	0.375360	0.001161	0.716465
-4.706381	-2.133277	0.380365	0.001086	0.716458
-5.035924	-2.071905	0.385370	0.001147	0.716463
-5.165177	-2.060509	0.390374	0.001171	0.716440
-5.514446	-2.150180	0.395379	0.001236	0.716140
-5.484694	-2.151775	0.400384	0.001230	0.716147
-6.160580	-2.034274	0.405389	0.001356	0.716142
-5.591275	-2.134484	0.410394	0.001250	0.716144
-5.716496	-2.169093	0.415398	0.001273	0.716031
-6.898322	-2.029487	0.420403	0.001493	0.715891
-6.363732	-2.123635	0.425408	0.001394	0.715893
-6.577690	-2.090881	0.430413	0.001433	0.715883
-6.690311	-2.064049	0.435418	0.001454	0.715896
-6.644849	-2.157696	0.440422	0.001446	0.715727
-7.852344	-2.031860	0.445427	0.001670	0.715550
-7.265662	-2.133478	0.450432	0.001561	0.715556
-7.857818	-2.033598	0.455437	0.001671	0.715545
-7.688195	-2.058259	0.460442	0.001640	0.715556
-7.361325	-2.119624	0.465446	0.001579	0.715550
-8.285092	-2.103308	0.470451	0.001751	0.715256
-8.522659	-2.065399	0.475456	0.001795	0.715248
-8.520911	-2.071688	0.480461	0.001794	0.715236
-8.313906	-2.104702	0.485466	0.001756	0.715244
-8.987212	-1.984777	0.490470	0.001881	0.715244
-8.833487	-2.007947	0.495475	0.001852	0.715253
-8.580558	-2.164185	0.500480	0.001805	0.715032
-10.140629	-1.945017	0.505485	0.002095	0.714916
-9.563238	-2.044595	0.510490	0.001988	0.714922
-9.289396	-2.098009	0.515494	0.001937	0.714913
-9.696018	-2.026329	0.520499	0.002012	0.714912
-9.543427	-2.050754	0.525504	0.001984	0.714918
-9.628780	-2.040701	0.530509	0.002000	0.714907
-10.160420	-2.088030	0.535514	0.002099	0.714626
-10.433732	-2.046185	0.540518	0.002149	0.714612
-10.494794	-2.036447	0.545523	0.002161	0.714610
-9.941569	-2.132824	0.550528	0.002058	0.714615
-10.497248	-2.036479	0.555533	0.002161	0.714609
-10.354029	-2.059355	0.560538	0.002134	0.714615
-10.231154	-2.157868	0.565542	0.002111	0.714463
-11.616735	-2.000323	0.570547	0.002369	0.714286
-11.362415	-2.044718	0.575552	0.002322	0.714288
-11.514245	-2.019048	0.580557	0.002350	0.714285
-11.213245	-2.068616	0.585562	0.002294	0.714293
-11.376243	-2.042566	0.590566	0.002324	0.714287
-11.647914	-1.994449	0.595571	0.002375	0.714287
-11.044099	-2.163198	0.600576	0.002262	0.714166
-12.284422	-2.038786	0.605581	0.002493	0.713974
-12.198828	-2.047945	0.610586	0.002477	0.713986
-12.367647	-2.021603	0.615590	0.002508	0.713979
-12.542670	-1.988933	0.620595	0.002541	0.713982
-12.273032	-2.032211	0.625600	0.002491	0.713992
-12.490467	-1.998465	0.630605	0.002531	0.713982
-12.206656	-2.092089	0.635610	0.002478	0.713896
-13.378995	-2.001251	0.640614	0.002696	0.713662
-13.176518	-2.036454	0.645619	0.002658	0.713664
-13.073607	-2.051527	0.650624	0.002639	0.713670
-13.357949	-2.005781	0.655629	0.002692	0.713661
-13.322461	-2.008884	0.660634	0.002685	0.713667
-13.259799	-2.020555	0.665638	0.002674	0.713667
-13.274974	-2.019460	0.670643	0.002676	0.713663
-13.559866	-2.098196	0.675648	0.002729	0.713406
-14.270717	-1.993575	0.680653	0.002862	0.713362
-13.912691	-2.047426	0.685658	0.002795	0.713382
-13.766926	-2.079197	0.690662	0.002768	0.713371
-14.188221	-2.004226	0.695667	0.002846	0.713371
-14.066550	-2.025389	0.700672	0.002823	0.713372
-14.065796	-2.029053	0.705677	0.002823	0.713365
-14.759835	-2.067353	0.710682	0.002952	0.713043
-15.052449	-2.021539	0.715686	0.003007	0.713031
-15.154627	-2.002159	0.720691	0.003026	0.713033
-14.699388	-2.082470	0.725696	0.002941	0.713035
-14.998091	-2.031925	0.730701	0.002996	0.713030
-14.762501	-2.068716	0.735706	0.002952	0.713040
-14.781684	-2.067533	0.740710	0.002956	0.713036
-15.911495	-2.021029	0.745715	0.003166	0.712728
-15.677685	-2.064717	0.750720	0.003122	0.712724
-15.919503	-2.024812	0.755725	0.003167	0.712718
-15.891072	-2.027172	0.760730	0.003162	0.712723
-15.930645	-2.024080	0.765734	0.003169	0.712716
-15.709542	-2.064682	0.770739	0.003128	0.712713
-15.644925	-2.071607	0.775744	0.003116	0.712723
-16.589974	-2.042154	0.780749	0.003292	0.712446
-16.670085	-2.052405	0.785754	0.003307	0.712398
-16.439202	-2.095220	0.790758	0.003264	0.712394
-16.605136	-2.063856	0.795763	0.003294	0.712398
-16.677481	-2.050184	0.800768	0.003308	0.712400
-16.968817	-2.002042	0.805773	0.003362	0.712392
-16.777777	-2.031100	0.810778	0.003326	0.712403
-17.051272	-2.091651	0.815782	0.003377	0.712185
-17.920526	-1.981823	0.820787	0.003539	0.712095
-17.713933	-2.015064	0.825792	0.003500	0.712103
-17.810675	-2.003271	0.830797	0.003518	0.712092
-17.676826	-2.021242	0.835802	0.003493	0.712104
-17.631068	-2.032016	0.840806	0.003485	0.712099
-17.883234	-1.988501	0.845811	0.003532	0.712096
-17.571975	-2.094928	0.850816	0.003474	0.711995
-18.501335	-2.043968	0.855821	0.003647	0.711766
-18.499996	-2.040761	0.860826	0.003646	0.711773
-18.924030	-1.968269	0.865830	0.003725	0.711767
-18.479193	-2.049045	0.870835	0.003642	0.711764
-18.416402	-2.056434	0.875840	0.003630	0.711772
-18.880859	-1.976584	0.880845	0.003717	0.711766
-18.628831	-2.031619	0.885850	0.003670	0.711746
-18.955827	-2.115079	0.890854	0.003731	0.711464
-19.641209	-1.995709	0.895859	0.003858	0.711459
-19.784259	-1.967132	0.900864	0.003885	0.711465
-19.555884	-2.011105	0.905869	0.003842	0.711459
-19.555499	-2.008473	0.910874	0.003842	0.711464
-19.556960	-2.008173	0.915878	0.003842	0.711464
-19.545861	-2.010815	0.920883	0.003840	0.711463
-19.547722	-2.127271	0.925888	0.003840	0.711230
-20.900314	-1.926329	0.930893	0.004092	0.711150
-20.616572	-1.972267	0.935898	0.004039	0.711160
-20.402830	-2.012928	0.940902	0.003999	0.711155
-21.075442	-1.891177	0.945907	0.004124	0.711159
-20.703108	-1.954580	0.950912	0.004055	0.711165
-20.417341	-2.011279	0.955917	0.004002	0.711153
-20.811630	-1.937511	0.960922	0.004075	0.711161
-21.006976	-2.031442	0.965926	0.004111	0.710904
-21.204710	-2.004380	0.970931	0.004148	0.710888
-21.219292	-2.000491	0.975936	0.004151	0.710890
-21.312308	-1.988570	0.980941	0.004168	0.710881
-21.317033	-1.982724	0.985946	0.004169	0.710891
-21.003610	-2.043959	0.990950	0.004110	0.710881
-21.158603	-2.048196	0.995955	0.004139	0.710817
-22.036707	-2.028032	1.000960	0.004302	0.710545
-22.072458	-2.026779	1.005965	0.004309	0.710535
-22.063545	-2.025242	1.010970	0.004307	0.710541
-22.270517	-1.989810	1.015974	0.004346	0.710539
-22.003797	-2.037722	1.020979	0.004296	0.710538
-22.166609	-2.005861	1.025984	0.004326	0.710544
-22.483713	-1.987838	1.030989	0.004385	0.710467
-22.881450	-2.038156	1.035994	0.004459	0.710225
-22.793664	-2.055242	1.040998	0.004443	0.710223
-23.337730	-1.957911	1.046003	0.004544	0.710223
-22.749235	-2.060189	1.051008	0.004434	0.710229
-22.916580	-2.034666	1.056013	0.004465	0.710220
-22.958762	-2.022582	1.061018	0.004473	0.710230
-23.277891	-2.021865	1.066022	0.004533	0.710118
-24.193827	-1.968352	1.071027	0.004703	0.709898
-23.589483	-2.074277	1.076032	0.004590	0.709902
-24.128131	-1.981110	1.081037	0.004691	0.709897
-24.121460	-1.979098	1.086042	0.004689	0.709903
-23.847912	-2.031506	1.091046	0.004638	0.709896
-24.138403	-1.979707	1.096051	0.004692	0.709896
-23.820046	-2.050130	1.101056	0.004633	0.709869
-24.519029	-2.062345	1.106061	0.004763	0.709596
-24.350431	-2.087860	1.111066	0.004732	0.709605
-24.830608	-2.004017	1.116070	0.004821	0.709601
-24.552100	-2.053486	1.121075	0.004769	0.709602
-24.337979	-2.088478	1.126080	0.004729	0.709608
-24.939472	-1.987192	1.131085	0.004841	0.709597
-24.768662	-2.113386	1.136090	0.004809	0.709405
-25.865732	-1.984508	1.141094	0.005013	0.709272
-25.651210	-2.022693	1.146099	0.004973	0.709272
-25.562920	-2.035929	1.151104	0.004957	0.709278
-25.789605	-2.001814	1.156109	0.004999	0.709265
-25.600473	-2.029549	1.161114	0.004963	0.709277
-25.779135	-2.002236	1.166118	0.004997	0.709268
-25.896930	-2.043004	1.171123	0.005019	0.709145
-26.544403	-2.017088	1.176128	0.005139	0.708966
-26.410359	-2.044091	1.181133	0.005114	0.708960
-26.831740	-1.965964	1.186138	0.005192	0.708966
-26.653052	-1.999091	1.191142	0.005159	0.708964
-26.460638	-2.035442	1.196147	0.005123	0.708960
-26.620064	-2.002785	1.201152	0.005153	0.708968
-26.727517	-2.017310	1.206157	0.005173	0.708901
-27.207232	-2.057096	1.211162	0.005262	0.708650
-27.421276	-2.020044	1.216166	0.005302	0.708648
-28.041417	-1.910239	1.221171	0.005417	0.708647
-27.123028	-2.069995	1.226176	0.005246	0.708655
-27.386320	-2.028103	1.231181	0.005295	0.708645
-27.535530	-1.999527	1.236186	0.005323	0.708649
-27.189345	-2.087198	1.241190	0.005258	0.708597
-28.200346	-2.025983	1.246195	0.005446	0.708359
-28.338280	-1.998405	1.251200	0.005472	0.708365
-28.647498	-1.948014	1.256205	0.005529	0.708356
-28.144241	-2.033838	1.261210	0.005435	0.708364
-28.326074	-2.000812	1.266214	0.005469	0.708365
-28.534582	-1.967044	1.271219	0.005508	0.708359
-28.118187	-2.050668	1.276224	0.005430	0.708340
-29.075328	-2.039948	1.281229	0.005609	0.708020
-29.407961	-1.976040	1.286234	0.005670	0.708029
-29.477872	-1.968018	1.291238	0.005683	0.708020
-29.128887	-2.028807	1.296243	0.005618	0.708023
-29.243973	-2.005223	1.301248	0.005640	0.708030
-29.544191	-1.957716	1.306253	0.005695	0.708018
-29.169830	-2.020030	1.311258	0.005626	0.708027
-29.524411	-2.075140	1.316262	0.005692	0.707790
-30.759853	-1.892091	1.321267	0.005921	0.707715
-30.358796	-1.962044	1.326272	0.005847	0.707718
-30.000168	-2.029727	1.331277	0.005780	0.707711
-30.446584	-1.947333	1.336282	0.005863	0.707717
-30.207801	-1.993192	1.341286	0.005818	0.707710
-30.123165	-2.011348	1.346291	0.005803	0.707704
-30.300769	-2.024509	1.351296	0.005836	0.707615
-31.409107	-1.942378	1.356301	0.006042	0.707383
-30.916600	-2.027659	1.361306	0.005950	0.707388
-31.184691	-1.981477	1.366310	0.006000	0.707385
-31.439479	-1.937509	1.371315	0.006047	0.707383
-31.045663	-2.000575	1.376320	0.005974	0.707397
-31.090282	-2.000283	1.381325	0.005982	0.707382
-31.153103	-1.986755	1.386330	0.005994	0.707387
-31.522150	-2.062142	1.391334	0.006062	0.707103
-31.739736	-2.030206	1.396339	0.006103	0.707090
-31.791374	-2.019370	1.401344	0.006112	0.707093
-31.884028	-2.007872	1.406349	0.006129	0.707083
-31.906452	-1.999716	1.411354	0.006134	0.707092
-31.889085	-2.005143	1.416358	0.006130	0.707087
-31.993721	-2.035929	1.421363	0.006150	0.706988
-32.780274	-2.008429	1.426368	0.006296	0.706762
-32.794167	-2.012285	1.431373	0.006299	0.706749
-32.959238	-1.977738	1.436378	0.006329	0.706760
-32.892240	-1.991270	1.441382	0.006317	0.706757
-32.961828	-1.981083	1.446387	0.006329	0.706753
-32.810243	-2.005612	1.451392	0.006301	0.706758
-32.924353	-1.993122	1.456397	0.006322	0.706742
-32.954597	-2.132055	1.461402	0.006328	0.706452
-33.411120	-2.052983	1.466406	0.006413	0.706448
-33.996033	-1.950796	1.471411	0.006522	0.706444
-33.428748	-2.049530	1.476416	0.006416	0.706449
-33.607882	-2.020516	1.481421	0.006449	0.706443
-33.814552	-1.980499	1.486426	0.006488	0.706450
-33.654182	-2.071978	1.491430	0.006458	0.706323
-34.533675	-2.010526	1.496435	0.006621	0.706132
-34.130396	-2.080615	1.501440	0.006546	0.706136
-34.747952	-1.975828	1.506445	0.006661	0.706125
-34.801305	-1.963331	1.511450	0.006671	0.706131
-34.241436	-2.061795	1.516454	0.006567	0.706134
-34.549080	-2.008051	1.521459	0.006624	0.706132
-34.612073	-2.066910	1.526464	0.006636	0.705991
-35.514014	-1.969983	1.531469	0.006803	0.705863
-35.325043	-2.000326	1.536474	0.006768	0.705870
-35.154888	-2.033640	1.541478	0.006736	0.705864
-35.609935	-1.953391	1.546483	0.006821	0.705862
-35.315735	-2.001519	1.551488	0.006766	0.705871
-35.457167	-1.981743	1.556493	0.006792	0.705861
-35.279783	-2.119410	1.561498	0.006759	0.705647
-36.129064	-2.029351	1.566502	0.006917	0.705524
-36.413327	-1.978259	1.571507	0.006970	0.705525
-36.367035	-1.981585	1.576512	0.006961	0.705535
-36.290313	-1.999951	1.581517	0.006947	0.705526
-36.090122	-2.033460	1.586522	0.006910	0.705530
-36.213648	-2.013228	1.591526	0.006933	0.705527
-36.767360	-2.043521	1.596531	0.007036	0.705267
-36.738183	-2.072946	1.601536	0.007030	0.705219
-37.197715	-1.994916	1.606541	0.007116	0.705211
-37.188850	-1.993667	1.611546	0.007114	0.705217
-37.212535	-1.989174	1.616550	0.007118	0.705218
-37.267481	-1.981124	1.621555	0.007128	0.705214
-36.955341	-2.032302	1.626560	0.007070	0.705223
-37.471597	-2.086724	1.631565	0.007166	0.704929
-38.172799	-1.977818	1.636570	0.007297	0.704896
-38.354756	-1.945928	1.641574	0.007330	0.704896
-38.002300	-2.011927	1.646579	0.007265	0.704889
-37.842661	-2.035074	1.651584	0.007235	0.704900
-38.231828	-1.970047	1.656589	0.007307	0.704892
-38.007266	-2.008950	1.661594	0.007265	0.704894
-38.012882	-2.103120	1.666598	0.007267	0.704702
-39.177848	-1.949028	1.671603	0.007483	0.704595
-38.865016	-2.001343	1.676608	0.007425	0.704602
-38.782136	-2.021150	1.681613	0.007409	0.704592
-38.905805	-1.997674	1.686618	0.007432	0.704595
-38.803825	-2.015116	1.691622	0.007413	0.704596
-38.931792	-1.994010	1.696627	0.007437	0.704593
-38.841599	-2.137383	1.701632	0.007420	0.704337
-39.948003	-1.978138	1.706637	0.007626	0.704260
-39.960606	-1.973608	1.711642	0.007628	0.704265
-39.407378	-2.073034	1.716646	0.007525	0.704263
-39.647476	-2.030469	1.721651	0.007570	0.704263
-39.803076	-2.001765	1.726656	0.007599	0.704265
-39.830221	-1.999675	1.731661	0.007604	0.704260
-40.473751	-2.027982	1.736666	0.007724	0.703972
-40.647615	-2.006778	1.741670	0.007756	0.703952
-40.703695	-1.997246	1.746675	0.007766	0.703951
-40.502204	-2.029526	1.751680	0.007729	0.703959
-40.745343	-1.990363	1.756685	0.007774	0.703950
-40.677875	-1.997786	1.761690	0.007761	0.703960
-40.211386	-2.083068	1.766694	0.007674	0.703956
-41.183731	-2.063175	1.771699	0.007855	0.703646
-41.700507	-1.972835	1.776704	0.007951	0.703643
-41.511692	-2.012795	1.781709	0.007916	0.703630
-41.171013	-2.070160	1.786714	0.007853	0.703637
-41.688559	-1.978986	1.791718	0.007949	0.703635
-41.953173	-1.932513	1.796723	0.007998	0.703634
-41.225058	-2.057124	1.801728	0.007862	0.703645
-41.917371	-2.068135	1.806733	0.007991	0.703373
-42.579173	-1.966086	1.811738	0.008114	0.703341
-42.255422	-2.021557	1.816742	0.008054	0.703346
-42.042841	-2.061964	1.821747	0.008014	0.703341
-42.117886	-2.045765	1.826752	0.008028	0.703347
-42.608410	-1.962189	1.831757	0.008119	0.703339
-42.209473	-2.048726	1.836762	0.008045	0.703308
-43.154281	-2.028486	1.841766	0.008221	0.703009
-43.451276	-1.978285	1.846771	0.008276	0.703004
-43.224441	-2.014434	1.851776	0.008234	0.703013
-43.033190	-2.054438	1.856781	0.008198	0.703001
-43.076760	-2.041418	1.861786	0.008206	0.703012
-42.878916	-2.077923	1.866790	0.008169	0.703009
-43.086211	-2.091264	1.871795	0.008208	0.702908
-44.129677	-2.009753	1.876800	0.008402	0.702697
-43.939292	-2.048520	1.881805	0.008367	0.702687
-43.766031	-2.074773	1.886810	0.008334	0.702697
-44.203624	-1.996146	1.891814	0.008416	0.702698
-44.269617	-1.987780	1.896819	0.008428	0.702691
-43.865942	-2.053218	1.901824	0.008353	0.702705
-43.978755	-2.109168	1.906829	0.008373	0.702551
-45.331190	-1.955072	1.911834	0.008625	0.702375
-44.927964	-2.027149	1.916838	0.008550	0.702375
-44.929553	-2.029491	1.921843	0.008550	0.702370
-45.143895	-1.986957	1.926848	0.008590	0.702379
-45.130435	-1.993293	1.931853	0.008587	0.702371
-44.991712	-2.015323	1.936858	0.008562	0.702377
-44.995467	-2.039932	1.941862	0.008562	0.702326
-45.890725	-2.002568	1.946867	0.008729	0.702079
-45.633157	-2.045940	1.951872	0.008681	0.702084
-45.995161	-1.986033	1.956877	0.008748	0.702075
-45.978002	-1.985543	1.961882	0.008745	0.702082
-45.828829	-2.013334	1.966886	0.008717	0.702080
-45.874180	-2.007756	1.971891	0.008725	0.702075
-45.805368	-2.042669	1.976896	0.008712	0.702029
-46.772090	-2.010552	1.981901	0.008892	0.701745
-46.491010	-2.057579	1.986906	0.008840	0.701752
-46.789776	-2.004739	1.991910	0.008895	0.701751
-47.063228	-1.958571	1.996915	0.008946	0.701746
-46.510793	-2.053156	2.001920	0.008843	0.701754

-46.769320	-2.038222	2.011917	0.008891	0.701691
-47.481832	-2.028995	2.021914	0.009024	0.701453
-47.882586	-1.959515	2.031910	0.009098	0.701450
-47.745561	-1.987264	2.041907	0.009073	0.701443
-47.601961	-2.012442	2.051904	0.009046	0.701444
-47.804817	-1.974115	2.061901	0.009083	0.701449
-47.615827	-1.975662	2.071898	0.009048	0.701514
-46.979462	-1.974353	2.081894	0.008929	0.701747
-46.765649	-2.013360	2.091891	0.008889	0.701746
-46.879272	-1.991637	2.101888	0.008910	0.701749
-46.755142	-2.013342	2.111885	0.008887	0.701750
-46.821189	-2.002185	2.121882	0.008899	0.701749
-46.876314	-1.993941	2.131878	0.008909	0.701746
-46.813189	-2.005234	2.141875	0.008897	0.701746
-46.811790	-1.959846	2.151872	0.008897	0.701839
-45.849471	-2.010795	2.161869	0.008718	0.702083
-45.900209	-2.005188	2.171866	0.008727	0.702077
-46.252624	-1.941550	2.181862	0.008792	0.702079
-45.844021	-2.016828	2.191859	0.008716	0.702074
-45.484138	-1.975557	2.201856	0.008649	0.702288
-45.270294	-1.969396	2.211853	0.008609	0.702378
-45.208493	-1.978945	2.221850	0.008597	0.702381
-45.198767	-1.983578	2.231846	0.008595	0.702375
-44.654138	-1.956096	2.241843	0.008494	0.702628
-44.277327	-1.988630	2.251840	0.008423	0.702698
-44.124069	-2.016764	2.261837	0.008395	0.702697
-44.129854	-2.015500	2.271834	0.008396	0.702697
-43.850074	-1.927399	2.281830	0.008343	0.702977
-43.276184	-2.011021	2.291827	0.008236	0.703015
-43.375792	-1.993303	2.301824	0.008255	0.703015
-43.369180	-1.958043	2.311821	0.008253	0.703089
-42.481748	-1.987933	2.321818	0.008088	0.703348
-42.408645	-2.003945	2.331814	0.008074	0.703342
-42.446555	-1.997612	2.341811	0.008081	0.703342
-42.207242	-1.956167	2.351808	0.008036	0.703512
-41.415616	-2.035726	2.361805	0.007889	0.703637
-41.625651	-1.997047	2.371802	0.007928	0.703639
-41.681670	-1.988997	2.381798	0.007938	0.703636
-40.903812	-1.977864	2.391795	0.007793	0.703938
-40.899063	-1.969297	2.401792	0.007792	0.703958
-40.480290	-2.044294	2.411789	0.007714	0.703957
-40.639058	-1.959008	2.421786	0.007743	0.704073
-39.759401	-2.021689	2.431782	0.007579	0.704263
-39.848925	-2.006042	2.441779	0.007596	0.704262
-39.799267	-2.014544	2.451776	0.007586	0.704263
-39.053240	-2.016975	2.461773	0.007447	0.704527
-39.037532	-1.986161	2.471770	0.007444	0.704595
-38.737844	-2.039075	2.481766	0.007388	0.704596
-38.999230	-1.971740	2.491763	0.007437	0.704639
-38.306292	-1.969442	2.501760	0.007308	0.704892
-37.820975	-2.055907	2.511757	0.007217	0.704893
-38.216307	-1.986838	2.521754	0.007290	0.704890
-37.566840	-1.989083	2.531750	0.007169	0.705119
-37.361681	-1.979083	2.541747	0.007131	0.705213
-37.387905	-1.973593	2.551744	0.007136	0.705215
-37.222899	-1.942807	2.561741	0.007105	0.705337
-36.373243	-1.997699	2.571738	0.006947	0.705531
-36.450691	-1.985602	2.581734	0.006961	0.705528
-36.517530	-1.971320	2.591731	0.006973	0.705533
-35.768145	-1.937890	2.601728	0.006833	0.705870
-35.150603	-2.046750	2.611725	0.006718	0.705873
-35.633206	-1.960696	2.621722	0.006808	0.705873
-35.263001	-1.969180	2.631718	0.006739	0.705989
-34.644185	-2.007118	2.641715	0.006623	0.706135
-34.664020	-2.002921	2.651712	0.006627	0.706136
-34.748294	-1.985686	2.661709	0.006642	0.706141
-33.966574	-1.969642	2.671706	0.006497	0.706454
-33.803121	-1.999977	2.681702	0.006466	0.706452
-33.919602	-1.980539	2.691699	0.006488	0.706449
-33.595317	-1.943610	2.701696	0.006427	0.706640
-32.797731	-2.024614	2.711693	0.006279	0.706763
-33.026352	-1.985035	2.721690	0.006321	0.706761
-32.879228	-1.982625	2.731686	0.006293	0.706819
-32.174695	-1.975118	2.741683	0.006162	0.707087
-32.116271	-1.985062	2.751680	0.006151	0.707088
-32.064018	-1.992777	2.761677	0.006141	0.707091
-31.657034	-1.953248	2.771674	0.006065	0.707317
-31.163757	-2.008063	2.781670	0.005973	0.707383
-31.426609	-1.963283	2.791667	0.006022	0.707380
-30.984172	-1.993070	2.801664	0.005939	0.707478
-30.365585	-1.989898	2.811661	0.005824	0.707706
-30.219368	-2.016032	2.821658	0.005797	0.707706
-30.433802	-1.977934	2.831654	0.005836	0.707706
-29.810512	-1.958259	2.841651	0.005720	0.707969
-29.507188	-1.988424	2.851648	0.005664	0.708017
-29.366595	-2.012659	2.861645	0.005637	0.708019
-29.500637	-1.920333	2.871642	0.005662	0.708157
-28.460197	-2.004070	2.881638	0.005468	0.708361
-28.406588	-2.016273	2.891635	0.005458	0.708356
-28.557766	-1.987890	2.901632	0.005486	0.708359
-27.885927	-2.000254	2.911629	0.005361	0.708575
-27.822442	-1.973731	2.921626	0.005349	0.708651
-27.758567	-1.986828	2.931622	0.005337	0.708648
-27.840907	-1.915903	2.941619	0.005352	0.708761
-26.989216	-1.960874	2.951616	0.005193	0.708975
-27.050107	-1.949476	2.961613	0.005204	0.708976
-27.051216	-1.931949	2.971610	0.005204	0.709011
-26.154379	-1.957632	2.981606	0.005037	0.709280
-26.160822	-1.956638	2.991603	0.005038	0.709280
-26.115803	-1.967079	3.001600	0.005030	0.709275
-25.500162	-1.951545	3.011597	0.004915	0.709526
-25.070429	-1.986556	3.021594	0.004835	0.709610
-25.284004	-1.949242	3.031590	0.004874	0.709609
-25.190678	-1.927431	3.041587	0.004857	0.709686
-24.249322	-1.986814	3.051584	0.004681	0.709903
-24.317106	-1.971296	3.061581	0.004694	0.709910
-24.511504	-1.936422	3.071578	0.004730	0.709911
-23.799110	-1.922485	3.081574	0.004597	0.710193
-23.351140	-1.981853	3.091571	0.004513	0.710234
-23.199995	-2.011675	3.101568	0.004485	0.710229
-23.494423	-1.912489	3.111565	0.004540	0.710322
-22.299717	-2.012913	3.121562	0.004317	0.710547
-22.684408	-1.948048	3.131558	0.004389	0.710540
-22.306826	-2.016063	3.141555	0.004318	0.710539
-21.936745	-1.975119	3.151552	0.004249	0.710753
-21.315952	-2.018847	3.161549	0.004133	0.710887
-21.571849	-1.971218	3.171546	0.004181	0.710891
-21.387751	-2.008321	3.181542	0.004146	0.710883
-21.132323	-1.943880	3.191539	0.004099	0.711103
-20.966064	-1.947857	3.201536	0.004067	0.711154
-20.895312	-1.960852	3.211533	0.004054	0.711154
-20.164922	-1.997121	3.221530	0.003918	0.711341
-20.227124	-1.924980	3.231526	0.003929	0.711464
-20.017704	-1.959468	3.241523	0.003890	0.711469
-19.910197	-1.942073	3.251520	0.003870	0.711543
-19.118894	-1.968291	3.261517	0.003723	0.711772
-19.047790	-1.980838	3.271514	0.003709	0.711772
-19.253834	-1.944442	3.281510	0.003747	0.711772
-18.468887	-1.943770	3.291507	0.003601	0.712053
-18.467966	-1.921037	3.301504	0.003601	0.712099
-18.355308	-1.940870	3.311501	0.003580	0.712099
-17.883278	-1.936581	3.321498	0.003492	0.712276
-17.667034	-1.912588	3.331494	0.003451	0.712401
-17.453225	-1.954676	3.341491	0.003411	0.712393
-17.565420	-1.890795	3.351488	0.003432	0.712481
-16.563210	-1.946490	3.361485	0.003245	0.712726
-16.649296	-1.932643	3.371482	0.003261	0.712723
-16.728930	-1.919946	3.381478	0.003276	0.712720
-16.006476	-1.901145	3.391475	0.003141	0.713014
-15.776320	-1.931582	3.401472	0.003098	0.713036
-15.583757	-1.966354	3.411469	0.003062	0.713035
-15.390702	-1.919231	3.421466	0.003026	0.713198
-14.837106	-1.930815	3.431462	0.002923	0.713371
-14.747306	-1.946966	3.441459	0.002906	0.713371
-14.743375	-1.949903	3.451456	0.002905	0.713367
-13.922492	-1.971278	3.461453	0.002752	0.713616
-14.086193	-1.914570	3.471450	0.002782	0.713671
-13.970384	-1.940148	3.481446	0.002760	0.713661
-13.684045	-1.950675	3.491443	0.002707	0.713742
-13.010092	-1.953865	3.501440	0.002581	0.713975
-12.691605	-2.008707	3.511437	0.002522	0.713979
-13.059128	-1.943317	3.521434	0.002590	0.713979
-12.536496	-1.938229	3.531430	0.002493	0.714174
-12.022838	-1.976118	3.541427	0.002397	0.714281
-12.285474	-1.925912	3.551424	0.002445	0.714288
-11.971607	-1.961914	3.561421	0.002387	0.714328
-11.267990	-1.941478	3.571418	0.002256	0.714618
-11.189700	-1.955145	3.581414	0.002241	0.714619
-11.046359	-1.982052	3.591411	0.002214	0.714617
-11.018939	-1.916646	3.601408	0.002209	0.714756
-9.912283	-2.028221	3.611405	0.002003	0.714927
-9.946802	-2.022069	3.621402	0.002009	0.714927
-9.779598	-2.055628	3.631398	0.001978	0.714920
-9.731223	-1.989945	3.641395	0.001968	0.715067
-8.973040	-2.036179	3.651392	0.001827	0.715244
-8.913548	-2.046614	3.661389	0.001816	0.715245
-8.900895	-2.048786	3.671386	0.001813	0.715245
-8.684031	-2.023399	3.681382	0.001773	0.715372
-7.920799	-2.067021	3.691379	0.001631	0.715556
-8.168397	-2.019215	3.701376	0.001677	0.715564
-7.974476	-2.057061	3.711373	0.001640	0.715557
-7.720501	-2.017482	3.721370	0.001593	0.715726
-6.666456	-2.120969	3.731366	0.001396	0.715893
-7.306022	-2.006781	3.741363	0.001515	0.715894
-6.762716	-2.103819	3.751360	0.001414	0.715894
-6.766480	-2.050352	3.761357	0.001415	0.715999
-6.200874	-2.077892	3.771354	0.001309	0.716144
-6.350099	-2.050563	3.781350	0.001337	0.716146
-6.326051	-2.056814	3.791347	0.001332	0.716142
-5.470906	-2.072467	3.801344	0.001173	0.716413
-5.406740	-2.060534	3.811341	0.001161	0.716460
-5.534780	-2.038911	3.821338	0.001184	0.716458
-4.885780	-2.129436	3.831334	0.001063	0.716508
-4.752971	-2.026039	3.841331	0.001038	0.716760
-4.319548	-2.102278	3.851328	0.000957	0.716762
-4.437908	-2.080485	3.861325	0.000979	0.716763
-3.780324	-2.096718	3.871322	0.000857	0.716963
-3.576238	-2.070152	3.881318	0.000819	0.717088
-3.530005	-2.079014	3.891315	0.000810	0.717087
-3.547733	-2.076091	3.901312	0.000813	0.717087
-2.832236	-2.052372	3.911309	0.000680	0.717387
-2.823530	-2.052220	3.921306	0.000678	0.717390
-2.675671	-2.079456	3.931302	0.000650	0.717389
-2.677856	-1.996990	3.941299	0.000650	0.717551
-2.549474	-1.940958	3.951296	0.000626	0.717708
-1.783015	-2.076378	3.961293	0.000483	0.717710
-2.286833	-1.900431	3.971290	0.000577	0.717881
-1.479072	-1.970603	3.981286	0.000426	0.718027
-1.580696	-1.952661	3.991283	0.000445	0.718027
-2.096416	-1.737807	4.001280	0.000541	0.718270
-1.427525	-1.808648	4.011277	0.000416	0.718366
-1.910360	-1.657771	4.021274	0.000506	0.718494
-1.036956	-1.730181	4.031270	0.000343	0.718659
-0.889651	-1.735982	4.041267	0.000316	0.718699
-1.762915	-1.436481	4.051264	0.000478	0.718984
-0.602498	-1.613999	4.061261	0.000262	0.719042
-0.887361	-1.438418	4.071258	0.000314	0.719288
-0.732583	-1.414626	4.081254	0.000285	0.719390
-1.103216	-1.231403	4.091251	0.000354	0.719621
-1.256731	-1.101394	4.101248	0.000383	0.719824
-0.873664	-1.090810	4.111245	0.000311	0.719980
-0.921333	-0.942902	4.121242	0.000320	0.720255
-0.773382	-0.855962	4.131238	0.000292	0.720478
-0.559497	-0.796683	4.141235	0.000252	0.720670
-0.407362	-0.712645	4.151232	0.000223	0.720889
-0.343650	-0.606315	4.161229	0.000211	0.721121
-0.476721	-0.475799	4.171226	0.000236	0.721331
-0.392322	-0.369742	4.181222	0.000220	0.721570
-0.332763	-0.250753	4.191219	0.000208	0.721825
-0.588919	-0.055149	4.201216	0.000256	0.722120
-0.182262	0.009985	4.211213	0.000180	0.722391
0.000000	0.173690	4.221210	0.000146	0.722776

0.024042	0.788991	4.226214	0.000141	0.723991
0.269148	2.001838	4.231219	0.000094	0.726450
0.808841	3.773992	4.236224	-0.000007	0.730090
1.100165	6.139957	4.241229	-0.000063	0.734773
1.711684	8.959133	4.246234	-0.000179	0.740405
2.296637	12.277166	4.251238	-0.000290	0.746934
2.681568	16.080238	4.256243	-0.000365	0.754252
3.489633	20.221586	4.261248	-0.000518	0.762269
4.153897	24.778131	4.266253	-0.000644	0.770920
4.924652	29.698862	4.271258	-0.000791	0.780172
6.407015	34.849150	4.276262	-0.001071	0.789953
8.027444	40.306315	4.281267	-0.001376	0.800202
10.051952	46.021755	4.286272	-0.001757	0.810897
10.996083	52.215510	4.291277	-0.001937	0.821949
12.165620	58.657549	4.296282	-0.002159	0.833343
13.105083	65.362406	4.301286	-0.002338	0.844957
13.737726	72.345012	4.306291	-0.002461	0.856783
14.247285	79.553902	4.311296	-0.002560	0.868781
14.720778	86.937185	4.316301	-0.002653	0.880886
15.220768	94.500947	4.321306	-0.002751	0.893121
15.696117	102.196249	4.326310	-0.002845	0.905390
16.283221	110.028028	4.331315	-0.002960	0.917735
16.786505	117.979113	4.336320	-0.003059	0.930076
17.216097	126.041447	4.341325	-0.003144	0.942403
17.640022	134.221502	4.346330	-0.003228	0.954744
18.246414	142.431306	4.351334	-0.003347	0.967017
18.783681	150.746377	4.356339	-0.003452	0.979272
19.117965	159.184567	4.361344	-0.003520	0.991500
19.640348	167.608972	4.366349	-0.003623	1.003605
20.419345	176.040727	4.371354	-0.003773	1.015639
21.046087	184.542348	4.376358	-0.003896	1.027591
21.628582	193.088567	4.381363	-0.004010	1.039455
22.216171	201.669783	4.386368	-0.004125	1.051234
22.602397	210.288359	4.391373	-0.004203	1.062886
23.261725	218.909515	4.396378	-0.004331	1.074476
24.165332	227.463261	4.401382	-0.004505	1.085909
24.766332	236.091147	4.406387	-0.004622	1.097251
25.838269	244.659295	4.411392	-0.004828	1.108504
27.116812	253.192298	4.416397	-0.005071	1.119644
27.954052	261.838975	4.421402	-0.005233	1.130720
28.291024	270.545705	4.426406	-0.005302	1.141657
29.075429	279.194727	4.431411	-0.005453	1.152514
29.788097	287.827030	4.436416	-0.005592	1.163233
30.008536	296.509486	4.441421	-0.005639	1.173813
30.658357	305.105412	4.446426	-0.005765	1.184282
31.796438	313.624900	4.451430	-0.005983	1.194668
32.111266	322.252959	4.456435	-0.006047	1.204926
32.648322	330.863256	4.461440	-0.006153	1.215120
33.293635	339.414604	4.466445	-0.006279	1.225183
34.180192	347.963605	4.471450	-0.006449	1.235208
34.734724	356.504050	4.476454	-0.006558	1.245077
35.253425	365.053182	4.481459	-0.006660	1.254872
35.924930	373.557881	4.486464	-0.006791	1.264570
36.795039	382.020247	4.491469	-0.006959	1.274184
37.689935	390.466475	4.496474	-0.007131	1.283712
38.377991	398.954387	4.501478	-0.007265	1.293177
39.047970	407.427143	4.506483	-0.007395	1.302553
39.424644	416.032369	4.511488	-0.007471	1.311952
40.021271	424.502374	4.516493	-0.007588	1.321179
40.477527	432.948204	4.521498	-0.007678	1.330290
41.149048	441.343442	4.526502	-0.007809	1.339323
41.884972	449.716002	4.531507	-0.007951	1.348284
42.857533	458.061454	4.536512	-0.008138	1.357197
43.130541	466.483114	4.541517	-0.008194	1.366011
43.430410	474.921017	4.546522	-0.008256	1.374789
44.025575	483.274467	4.551526	-0.008372	1.383474
44.408365	491.679073	4.556531	-0.008449	1.392122
45.218716	499.990637	4.561536	-0.008605	1.400694
45.803175	508.317107	4.566541	-0.008720	1.409190
46.482428	516.649589	4.571546	-0.008852	1.417657
46.870839	525.004144	4.576550	-0.008929	1.426048
47.393922	533.337209	4.581555	-0.009032	1.434390
48.102027	541.636699	4.586560	-0.009170	1.442681
48.531400	549.963544	4.591565	-0.009255	1.450906
49.038203	558.279308	4.596570	-0.009355	1.459086
49.527014	566.576283	4.601574	-0.009451	1.467199
49.943092	574.937528	4.606579	-0.009534	1.475317
50.390260	583.219947	4.611584	-0.009623	1.483321
50.509061	591.550667	4.616589	-0.009651	1.491276
51.322515	599.759705	4.621594	-0.009808	1.499182
51.797925	608.024136	4.626598	-0.009902	1.507045
52.263667	616.300777	4.631603	-0.009994	1.514878
52.818793	624.555552	4.636608	-0.010103	1.522663
53.299747	632.806881	4.641613	-0.010198	1.530394
53.586232	641.100123	4.646618	-0.010257	1.538096
54.243684	649.314795	4.651622	-0.010384	1.545742
54.848491	657.564298	4.656627	-0.010503	1.553375
55.199177	665.818333	4.661632	-0.010573	1.560936
55.725499	674.023181	4.666637	-0.010677	1.568443
56.108236	682.288218	4.671642	-0.010753	1.575946
56.597391	690.500137	4.676646	-0.010850	1.583382
57.064770	698.721665	4.681651	-0.010942	1.590788
57.489508	706.967828	4.686656	-0.011027	1.598175
58.080009	715.136946	4.691661	-0.011142	1.605484
58.416294	723.393454	4.696666	-0.011210	1.612801
58.960422	731.588769	4.701670	-0.011317	1.620059
59.099410	739.840882	4.706675	-0.011348	1.627279
59.660884	748.102411	4.711680	-0.011458	1.634533
60.057020	756.265225	4.716685	-0.011538	1.641646
60.539654	764.443623	4.721690	-0.011633	1.648755
61.010991	772.634692	4.726694	-0.011726	1.655841
61.758715	780.763653	4.731699	-0.011871	1.662882
62.319518	788.957015	4.736704	-0.011981	1.669923
62.626316	797.168921	4.741709	-0.012043	1.676915
62.802106	805.383687	4.746714	-0.012081	1.683863
63.266556	813.564466	4.751718	-0.012173	1.690793
63.563023	821.765809	4.756723	-0.012234	1.697688
63.997871	829.942228	4.761728	-0.012320	1.704554
64.239236	838.151063	4.766733	-0.012371	1.711393
64.749823	846.312650	4.771738	-0.012471	1.718201
65.296645	854.449206	4.776742	-0.012578	1.724966
65.868251	862.604302	4.781747	-0.012690	1.731722
66.485151	870.764278	4.786752	-0.012810	1.738462
66.935342	878.902258	4.791757	-0.012900	1.745137
67.180527	887.127266	4.796762	-0.012951	1.751831
67.445119	895.311218	4.801766	-0.013005	1.758468
67.956174	903.419713	4.806771	-0.013106	1.765050
68.368464	911.594693	4.811776	-0.013188	1.771649
68.708061	919.759952	4.816781	-0.013257	1.778207
69.095475	927.908957	4.821786	-0.013334	1.784733
69.635704	936.073008	4.826790	-0.013440	1.791266
70.251416	944.216505	4.831795	-0.013560	1.797768
70.637654	952.351803	4.836800	-0.013637	1.804212
71.038055	960.493447	4.841805	-0.013717	1.810640
71.384296	968.658166	4.846810	-0.013787	1.817056
71.588568	976.826532	4.851814	-0.013831	1.823436
71.918181	984.960888	4.856819	-0.013897	1.829781
72.496746	993.090647	4.861824	-0.014011	1.836131
72.759302	1001.225695	4.866829	-0.014065	1.842426
73.112835	1009.371028	4.871834	-0.014136	1.848717
73.599943	1017.513603	4.876838	-0.014232	1.855001
74.151949	1025.594946	4.881843	-0.014340	1.861224
74.651130	1033.731281	4.886848	-0.014439	1.867461
75.458105	1041.833117	4.891853	-0.014594	1.873688
76.079314	1049.933114	4.896858	-0.014715	1.879870
76.481595	1058.067235	4.901862	-0.014796	1.886033
76.961006	1066.200999	4.906867	-0.014890	1.892184
77.260164	1074.381896	4.911872	-0.014951	1.898330
77.629969	1082.492613	4.916877	-0.015026	1.904412
77.950371	1090.651823	4.921882	-0.015091	1.910504
78.511277	1098.767267	4.926886	-0.015200	1.916572
78.744399	1106.900296	4.931891	-0.015249	1.922597
79.169047	1115.032563	4.936896	-0.015334	1.928623
79.599774	1123.145810	4.941901	-0.015419	1.934618
79.966865	1131.261227	4.946906	-0.015493	1.940588
80.232970	1139.414978	4.951910	-0.015548	1.946557
80.621900	1147.561189	4.956915	-0.015626	1.952515
81.139336	1155.671096	4.961920	-0.015727	1.958443
81.432101	1163.749288	4.966925	-0.015787	1.964306
81.804730	1171.852134	4.971930	-0.015862	1.970177
82.264781	1179.955569	4.976934	-0.015953	1.976041
82.566400	1188.062261	4.981939	-0.016015	1.981872
82.837296	1196.188905	4.986944	-0.016070	1.987698
83.397432	1204.282865	4.991949	-0.016180	1.993513
83.638199	1212.413670	4.996954	-0.016230	1.999304
83.969255	1220.508257	5.001958	-0.016297	2.005062
84.317963	1228.604286	5.006963	-0.016368	2.010806
84.869940	1236.714450	5.011968	-0.016476	2.016565
85.041176	1244.836159	5.016973	-0.016513	2.022276
85.456679	1252.931389	5.021978	-0.016596	2.027978
85.701757	1261.103070	5.026982	-0.016647	2.033699
85.912174	1269.196249	5.031987	-0.016691	2.039346
86.299953	1277.263271	5.036992	-0.016769	2.044978
86.661697	1285.339938	5.041997	-0.016841	2.050597
86.871842	1293.471440	5.047002	-0.016886	2.056224
87.356343	1301.535548	5.052006	-0.016982	2.061817
87.698265	1309.629979	5.057011	-0.017051	2.067401
88.485667	1317.695200	5.062016	-0.017203	2.072994
88.542870	1325.827602	5.067021	-0.017219	2.078545
88.854137	1333.911356	5.072026	-0.017282	2.084073
89.397009	1342.005140	5.077030	-0.017388	2.089617
89.916877	1350.078905	5.082035	-0.017490	2.095129
90.227466	1358.204858	5.087040	-0.017554	2.100642
90.682913	1366.270870	5.092045	-0.017644	2.106114
90.842566	1374.445841	5.097050	-0.017679	2.111616
90.949490	1382.609009	5.102054	-0.017704	2.117091
91.289315	1390.640055	5.107059	-0.017773	2.122486
91.933183	1398.694137	5.112064	-0.017898	2.127912
92.253185	1406.776916	5.117069	-0.017963	2.133312
92.425645	1414.885529	5.122074	-0.018000	2.138701
93.073735	1422.912181	5.127078	-0.018126	2.144067
93.432143	1430.991345	5.132083	-0.018199	2.149427
93.928296	1439.098409	5.137088	-0.018296	2.154805
94.157665	1447.166195	5.142093	-0.018344	2.160119
94.499243	1455.255748	5.147098	-0.018413	2.165445
94.863997	1463.355729	5.152102	-0.018487	2.170766
95.045618	1471.466809	5.157107	-0.018526	2.176064
95.458776	1479.541670	5.162112	-0.018608	2.181347
95.510652	1487.652081	5.167117	-0.018623	2.186608
95.824210	1495.762760	5.172122	-0.018687	2.191879
96.311552	1503.823377	5.177126	-0.018783	2.197122
96.550931	1511.888504	5.182131	-0.018833	2.202332
96.949274	1519.953969	5.187136	-0.018912	2.207544
97.199234	1528.052079	5.192141	-0.018964	2.212752
97.677050	1536.119152	5.197146	-0.019058	2.217948
97.833776	1544.215412	5.202150	-0.019093	2.223122
98.001782	1552.303519	5.207155	-0.019130	2.228279
98.341117	1560.401598	5.212160	-0.019198	2.233446
98.576663	1568.461551	5.217165	-0.019247	2.238568
98.862469	1576.525720	5.222170	-0.019306	2.243685
99.275695	1584.594267	5.227174	-0.019388	2.248804
99.700900	1592.660948	5.232179	-0.019473	2.253911
100.299076	1600.706304	5.237184	-0.019589	2.259008
100.652092	1608.770753	5.242189	-0.019661	2.264085
100.959074	1616.870196	5.247194	-0.019723	2.269167
101.089449	1625.069873	5.252198	-0.019753	2.274286
101.169315	1633.134412	5.257203	-0.019773	2.279305
102.158680	1641.091305	5.262208	-0.019962	2.284323
102.707344	1649.124472	5.267213	-0.020070	2.289340
102.941047	1657.244974	5.272218	-0.020119	2.294374
103.112450	1665.328352	5.277222	-0.020156	2.299368
103.609464	1673.359687	5.282227	-0.020254	2.304346
103.877197	1681.467610	5.287232	-0.020309	2.309341
104.102865	1689.557920	5.292237	-0.020357	2.314312
104.637565	1697.596797	5.297242	-0.020461	2.319265
104.996582	1705.657153	5.302246	-0.020534	2.324207
105.165230	1713.751033	5.307251	-0.020570	2.329143
105.884974	1721.790246	5.312256	-0.020710	2.334080
106.132160	1729.868706	5.317261	-0.020761	2.338992
106.474306	1737.930787	5.322266	-0.020830	2.343892
106.535233	1746.043318	5.327270	-0.020847	2.348788
106.810883	1754.125419	5.332275	-0.020903	2.353674
107.172999	1762.196988	5.337280	-0.020976	2.358549
107.352858	1770.235193	5.342285	-0.021015	2.363381
107.700311	1778.294901	5.347290	-0.021085	2.368228
108.249289	1786.369473	5.352294	-0.021193	2.373091
108.189105	1794.465700	5.357299	-0.021187	2.377907
108.719737	1802.497456	5.362304	-0.021291	2.382723
108.993186	1810.549875	5.367309	-0.021347	2.387521
109.297902	1818.639593	5.372314	-0.021409	2.392333
109.559119	1826.710079	5.377318	-0.021463	2.397122
109.910545	1834.740628	5.382323	-0.021534	2.401884
110.441415	1842.790358	5.387328	-0.021638	2.406661
110.443171	1850.907160	5.392333	-0.021644	2.411428
110.831937	1858.961612	5.397338	-0.021722	2.416178
111.194982	1867.014744	5.402342	-0.021794	2.420916
111.455689	1875.066089	5.407347	-0.021848	2.425636
111.531008	1883.187227	5.412352	-0.021868	2.430373
111.832128	1891.324122	5.417357	-0.021929	2.435128
112.121740	1899.328130	5.422362	-0.021988	2.439795
112.234895	1907.380250	5.427366	-0.022015	2.444467
112.383120	1915.438942	5.432371	-0.022048	2.449138
112.890161	1923.481630	5.437376	-0.022147	2.453816
113.227194	1931.507674	5.442381	-0.022216	2.458464
113.454820	1939.568019	5.447386	-0.022263	2.463114
113.604394	1947.656638	5.452390	-0.022296	2.467766
113.774006	1955.720367	5.457395	-0.022333	2.472396
114.235330	1963.751899	5.462400	-0.022425	2.477021
114.515714	1971.798917	5.467405	-0.022482	2.481633
115.216242	1979.808095	5.472410	-0.022618	2.486245
115.500229	1987.899891	5.477414	-0.022676	2.490865
115.947086	1995.951739	5.482419	-0.022765	2.495465
116.391093	2004.013588	5.487424	-0.022853	2.500063
116.418701	2012.098234	5.492429	-0.022863	2.504634
116.710819	2020.164819	5.497434	-0.022923	2.509207
117.164238	2028.258091	5.502438	-0.023013	2.513797
117.121414	2036.323804	5.507443	-0.023010	2.518328
117.311834	2044.385349	5.512448	-0.023051	2.522865
117.619755	2052.394096	5.517453	-0.023113	2.527373
118.119121	2060.432908	5.522458	-0.023212	2.531903
118.242802	2068.524159	5.527462	-0.023240	2.536427
118.661176	2076.510334	5.532467	-0.023323	2.540906
119.075854	2084.575675	5.537472	-0.023406	2.545420
119.009343	2092.664470	5.542477	-0.023399	2.549906
119.546948	2100.683760	5.547482	-0.023504	2.554387
119.769956	2108.764817	5.552486	-0.023551	2.558873
120.042118	2116.777046	5.557491	-0.023607	2.563316
120.375200	2124.846420	5.562496	-0.023674	2.567787
120.646120	2132.921417	5.567501	-0.023730	2.572249
121.015793	2140.978312	5.572506	-0.023804	2.576701
120.875495	2149.097014	5.577510	-0.023784	2.581143
121.188591	2157.094436	5.582515	-0.023847	2.585542
121.759111	2165.151871	5.587520	-0.023959	2.589984
121.819630	2173.425979	5.592525	-0.023976	2.594502
121.937921	2181.421624	5.597530	-0.024003	2.598865
122.430524	2189.364151	5.602534	-0.024100	2.603216
122.664557	2197.386609	5.607539	-0.024149	2.607586
122.724773	2205.459200	5.612544	-0.024165	2.611964
123.128018	2213.474939	5.617549	-0.024246	2.616327
123.473602	2221.494361	5.622554	-0.024315	2.620681
123.751414	2229.535111	5.627558	-0.024372	2.625034
123.969000	2237.574739	5.632563	-0.024418	2.629376
124.596174	2245.613509	5.637568	-0.024540	2.633737
124.772105	2253.668060	5.642573	-0.024578	2.638069
124.987537	2261.701955	5.647578	-0.024624	2.642386
125.187106	2269.780868	5.652582	-0.024666	2.646719
125.282865	2277.844265	5.657587	-0.024690	2.651029
125.624764	2285.909605	5.662592	-0.024759	2.655350
125.795098	2293.942816	5.667597	-0.024796	2.659635
126.141167	2301.969503	5.672602	-0.024865	2.663921
126.443712	2310.047013	5.677606	-0.024927	2.668225
126.524862	2318.119130	5.682611	-0.024947	2.672504
126.991517	2326.177130	5.687616	-0.025040	2.676794
127.346401	2334.177769	5.692621	-0.025111	2.681039
127.422646	2342.206508	5.697626	-0.025131	2.685275
127.979274	2350.243620	5.702630	-0.025240	2.689538
128.136130	2358.328762	5.707635	-0.025274	2.693795
128.527750	2366.365273	5.712640	-0.025352	2.698035
128.720300	2374.398519	5.717645	-0.025393	2.702253
129.024995	2382.438203	5.722650	-0.025456	2.706475
129.329317	2390.524792	5.727654	-0.025518	2.710715
129.563288	2398.561267	5.732659	-0.025566	2.714918
129.931398	2406.615399	5.737664	-0.025640	2.719132
130.139808	2414.627242	5.742669	-0.025684	2.723307
130.305452	2422.668023	5.747674	-0.025721	2.727489
130.578635	2430.766428	5.752678	-0.025777	2.731700
130.536916	2438.853083	5.757683	-0.025774	2.735879
130.885445	2446.854013	5.762688	-0.025845	2.740032
131.306057	2454.848497	5.767693	-0.025928	2.744179
131.589532	2462.903008	5.772698	-0.025986	2.748343
131.958530	2471.006671	5.777702	-0.026060	2.752530
132.142198	2479.081298	5.782707	-0.026100	2.756685
132.609367	2487.078354	5.787712	-0.026192	2.760811
132.832265	2495.082590	5.792717	-0.026239	2.764920
132.709615	2503.174013	5.797722	-0.026221	2.769047
133.021610	2511.235429	5.802726	-0.026285	2.773178
133.498224	2519.224907	5.807731	-0.026379	2.777276
133.619020	2527.298451	5.812736	-0.026407	2.781389
133.852548	2535.311912	5.817741	-0.026456	2.785473
134.200378	2543.351782	5.822746	-0.026526	2.789571
134.612925	2551.408549	5.827750	-0.026608	2.793674
134.778364	2559.440376	5.832755	-0.026644	2.797745
135.066253	2567.502715	5.837760	-0.026703	2.801833
135.569648	2575.475409	5.842765	-0.026802	2.805881
135.710452	2583.547394	5.847770	-0.026833	2.809953
135.985877	2591.626336	5.852774	-0.026890	2.814030
136.147082	2599.662983	5.857779	-0.026925	2.818073
136.429436	2607.701195	5.862784	-0.026983	2.822118
136.943580	2615.697879	5.867789	-0.027084	2.826150
137.288940	2623.747335	5.872794	-0.027154	2.830193
137.631062	2631.842674	5.877798	-0.027223	2.834252
137.645281	2639.890406	5.882803	-0.027231	2.838264
138.025306	2647.912582	5.887808	-0.027307	2.842277
138.185594	2655.952881	5.892813	-0.027342	2.846282
138.358772	2663.993074	5.897818	-0.027380	2.850282
138.650362	2672.057198	5.902822	-0.027439	2.854294
139.050149	2680.050612	5.907827	-0.027519	2.858272
139.358821	2688.114281	5.912832	-0.027582	2.862274
139.565457	2696.142580	5.917837	-0.027626	2.866247
139.734933	2704.185022	5.922842	-0.027663	2.870219
139.972086	2712.266716	5.927846	-0.027712	2.874209
140.219640	2720.288686	5.932851	-0.027764	2.878165
140.578947	2728.327885	5.937856	-0.027836	2.882129
140.801071	2736.354680	5.942861	-0.027882	2.886075
140.882577	2744.403684	5.947866	-0.027903	2.890018
141.238293	2752.469875	5.952870	-0.027975	2.893979
141.583339	2760.474240	5.957875	-0.028044	2.897904
141.835733	2768.528056	5.962880	-0.028096	2.901843
142.005687	2776.568642	5.967885	-0.028133	2.905766
142.499406	2784.562821	5.972890	-0.028231	2.909677
142.534069	2792.742524	5.977894	-0.028242	2.913650
142.699927	2800.752146	5.982899	-0.028279	2.917541
142.991576	2808.773032	5.987904	-0.028338	2.921439
143.330630	2816.738240	5.992909	-0.028407	2.925307
143.661320	2824.746150	5.997914	-0.028474	2.929191
143.855258	2832.843215	6.002918	-0.028515	2.933105
144.209653	2840.852722	6.007923	-0.028586	2.936980
144.667648	2848.873498	6.012928	-0.028677	2.940861
144.641021	2856.922296	6.017933	-0.028677	2.944724
144.933870	2864.959619	6.022938	-0.028737	2.948594
145.291582	2873.009168	6.027942	-0.028809	2.952468
145.360011	2881.070496	6.032947	-0.028827	2.956327
145.390867	2889.125500	6.037952	-0.028838	2.960177
145.926319	2897.116096	6.042957	-0.028943	2.964016
146.133712	2905.134004	6.047962	-0.028987	2.967847
146.618191	2913.189329	6.052966	-0.029083	2.971704
146.658666	2921.261849	6.057971	-0.029095	2.975543
147.163626	2929.266550	6.062976	-0.029195	2.979367
147.423617	2937.275473	6.067981	-0.029249	2.983176
147.869363	2945.296910	6.072986	-0.029337	2.986996
147.860320	2953.403959	6.077990	-0.029340	2.990828
148.224826	2961.436397	6.082995	-0.029414	2.994639
148.544439	2969.465437	6.088000	-0.029479	2.998441
148.701305	2977.484119	6.093005	-0.029513	3.002225
148.954835	2985.482953	6.098010	-0.029566	3.006000
148.999101	2993.553769	6.103014	-0.029579	3.009793
149.442632	3001.590458	6.108019	-0.029667	3.013585
149.809652	3009.626815	6.113024	-0.029741	3.017369
150.001971	3017.684950	6.118029	-0.029782	3.021149
150.244713	3025.670522	6.123034	-0.029832	3.024894
150.725340	3033.722453	6.128038	-0.029927	3.028676
150.998627	3041.768624	6.133043	-0.029983	3.032440
151.376736	3049.814126	6.138048	-0.030059	3.036205
151.367756	3057.839830	6.143053	-0.030063	3.039937
151.595877	3065.859767	6.148058	-0.030110	3.043673
152.056133	3073.912328	6.153062	-0.030202	3.047430
152.085244	3081.967990	6.158067	-0.030212	3.051164
152.356928	3090.026974	6.163072	-0.030268	3.054907
152.282124	3098.090110	6.168077	-0.030260	3.058630
152.914269	3106.055866	6.173082	-0.030383	3.062337
153.233177	3114.091898	6.178086	-0.030447	3.066057
153.305762	3122.114684	6.183091	-0.030466	3.069755
153.895440	3130.215057	6.188096	-0.030581	3.073509
154.143378	3138.250691	6.193101	-0.030633	3.077212
154.474706	3146.237349	6.198106	-0.030700	3.080892
154.709254	3154.240065	6.203110	-0.030749	3.084570
154.938999	3162.256356	6.208115	-0.030797	3.088250
155.240063	3170.345563	6.213120	-0.030858	3.091962
155.347803	3178.395585	6.218125	-0.030884	3.095643
155.775842	3186.371213	6.223130	-0.030969	3.099300
155.837696	3194.439611	6.228134	-0.030985	3.102978
156.049844	3202.449809	6.233139	-0.031030	3.106632
156.056356	3210.529147	6.238144	-0.031037	3.110305
156.453582	3218.565572	6.243149	-0.031116	3.113970
156.491254	3226.623112	6.248154	-0.031128	3.117625
156.877904	3234.608793	6.253158	-0.031206	3.121259
157.123967	3242.581225	6.258163	-0.031257	3.124876
157.522600	3250.619938	6.263168	-0.031336	3.128526
157.648077	3258.714425	6.268173	-0.031365	3.132184
157.555197	3266.796159	6.273178	-0.031353	3.135823
158.169367	3274.762660	6.278182	-0.031473	3.139437
158.181272	3282.798070	6.283187	-0.031480	3.143051
158.435822	3290.842083	6.288192	-0.031533	3.146675
158.924828	3298.831661	6.293197	-0.031629	3.150281
159.006777	3306.933526	6.298202	-0.031650	3.153915
159.254283	3314.965269	6.303206	-0.031701	3.157521
159.398069	3322.956250	6.308211	-0.031733	3.161100
159.794837	3330.955082	6.313216	-0.031813	3.164689
159.948887	3338.996336	6.318221	-0.031847	3.168283
160.096709	3347.050207	6.323226	-0.031879	3.171878
160.420413	3355.108391	6.328230	-0.031945	3.175479
160.969236	3363.051095	6.333235	-0.032052	3.179033
161.218689	3371.132806	6.338240	-0.032104	3.182632
161.354496	3379.143057	6.343245	-0.032135	3.186191
161.384447	3387.235843	6.348250	-0.032146	3.189778
161.845299	3395.286350	6.353254	-0.032237	3.193360
162.010169	3403.290028	6.358259	-0.032273	3.196905
162.342784	3411.309490	6.363264	-0.032340	3.200460
162.531905	3419.323223	6.368269	-0.032381	3.204003
163.004565	3427.353319	6.373274	-0.032474	3.207560
163.216148	3435.401436	6.378278	-0.032519	3.211111
163.248374	3443.446931	6.383283	-0.032530	3.214649
163.493366	3451.512036	6.388288	-0.032581	3.218201
163.667097	3459.525166	6.393293	-0.032619	3.221723
163.915918	3467.503102	6.398298	-0.032670	3.225228
164.433454	3475.567695	6.403302	-0.032772	3.228779
164.521654	3483.612583	6.408307	-0.032794	3.232300
164.985921	3491.683053	6.413312	-0.032886	3.235843
165.263157	3499.667424	6.418317	-0.032942	3.239337
165.569999	3507.647799	6.423322	-0.033005	3.242827
165.741234	3515.711810	6.428326	-0.033042	3.246344
165.888729	3523.705651	6.433331	-0.033075	3.249825
166.252123	3531.748824	6.438336	-0.033148	3.253333
166.177629	3539.817040	6.443341	-0.033139	3.256831
166.498786	3547.798073	6.448346	-0.033204	3.260302
166.891113	3555.819555	6.453350	-0.033283	3.263791
167.054044	3563.856880	6.458355	-0.033318	3.267273
167.358568	3571.904526	6.463360	-0.033380	3.270761
167.736946	3579.959325	6.468365	-0.033456	3.274252
167.966412	3587.976899	6.473370	-0.033504	3.277717
168.230515	3596.012297	6.478374	-0.033559	3.281188
168.618706	3603.961708	6.483379	-0.033636	3.284622
168.857978	3612.018004	6.488384	-0.033686	3.288093
168.928577	3620.080523	6.493389	-0.033705	3.291557
169.266987	3628.102235	6.498394	-0.033773	3.295009
169.567261	3636.162902	6.503398	-0.033834	3.298474
169.700826	3644.165944	6.508403	-0.033864	3.301903
170.046076	3652.190809	6.513408	-0.033934	3.305346
170.368827	3660.229128	6.518413	-0.033999	3.308791
170.223723	3668.298877	6.523418	-0.033978	3.312228
170.504017	3676.356430	6.528422	-0.034035	3.315671
171.001898	3684.302896	6.533427	-0.034133	3.319073
171.353675	3692.338120	6.538432	-0.034204	3.322502
171.459143	3700.333461	6.543437	-0.034229	3.325903
171.620995	3708.394702	6.548442	-0.034264	3.329329
171.841035	3716.448225	6.553446	-0.034311	3.332751
172.185449	3724.461002	6.558451	-0.034380	3.336157
172.421779	3732.501087	6.563456	-0.034429	3.339567
172.683848	3740.503680	6.568461	-0.034484	3.342958
172.692947	3748.532610	6.573466	-0.034491	3.346348
172.932074	3756.585487	6.578470	-0.034540	3.349753
173.071752	3764.619614	6.583475	-0.034572	3.353143
173.284018	3772.678747	6.588480	-0.034617	3.356543
173.608915	3780.665233	6.593485	-0.034682	3.359912
173.878931	3788.661593	6.598490	-0.034738	3.363280
174.197525	3796.708880	6.603494	-0.034803	3.366668
174.168543	3804.741714	6.608499	-0.034802	3.370035
174.688863	3812.785381	6.613504	-0.034905	3.373421
175.040900	3820.809763	6.618509	-0.034976	3.376791
175.283456	3828.799971	6.623514	-0.035026	3.380138
175.277388	3836.876698	6.628518	-0.035030	3.383510
175.708406	3844.876959	6.633523	-0.035116	3.386862
176.172441	3852.916336	6.638528	-0.035207	3.390228
176.116556	3861.038024	6.643533	-0.035202	3.393606
176.375884	3869.067967	6.648538	-0.035256	3.396954
176.873117	3877.005024	6.653542	-0.035354	3.400269
176.965054	3885.011450	6.658547	-0.035376	3.403595
177.163003	3893.040363	6.663552	-0.035418	3.406930
177.363029	3901.055958	6.668557	-0.035461	3.410257
177.617472	3909.089354	6.673562	-0.035514	3.413590
177.805188	3917.137709	6.678566	-0.035554	3.416923
178.067231	3925.144074	6.683571	-0.035608	3.420238
178.261541	3933.179761	6.688576	-0.035650	3.423560
178.574895	3941.181837	6.693581	-0.035713	3.426869
178.969551	3949.200373	6.698586	-0.035792	3.430184
179.389604	3957.279475	6.703590	-0.035876	3.433521
179.472590	3965.279861	6.708595	-0.035896	3.436812
179.539800	3973.315099	6.713600	-0.035914	3.440113
180.037029	3981.312866	6.718605	-0.036012	3.443410
180.092927	3989.361551	6.723610	-0.036028	3.446710
180.499447	3997.366284	6.728614	-0.036109	3.450000
180.430925	4005.415998	6.733619	-0.036101	3.453290
180.881541	4013.479438	6.738624	-0.036191	3.456599
181.261469	4021.473033	6.743629	-0.036267	3.459875
181.288409	4029.509237	6.748634	-0.036277	3.463153
181.858663	4037.541584	6.753638	-0.036388	3.466444
181.914889	4045.564026	6.758643	-0.036404	3.469711
182.029482	4053.635562	6.763648	-0.036431	3.472997
182.586249	4061.655528	6.768653	-0.036540	3.476273
182.840622	4069.637717	6.773658	-0.036593	3.479520
183.055540	4077.679867	6.778662	-0.036638	3.482788
183.027739	4085.682258	6.783667	-0.036638	3.486029
183.209229	4093.694366	6.788672	-0.036677	3.489278
183.423521	4101.765565	6.793677	-0.036722	3.492548
183.820811	4109.761488	6.798682	-0.036802	3.495790
184.011330	4117.764704	6.803686	-0.036842	3.499026
184.142782	4125.787709	6.808691	-0.036872	3.502265
184.188421	4133.814707	6.813696	-0.036886	3.505500
184.594943	4141.848722	6.818701	-0.036967	3.508746
184.799623	4149.908094	6.823706	-0.037010	3.511993
185.074039	4157.938622	6.828710	-0.037067	3.515228
185.406513	4165.927138	6.833715	-0.037134	3.518444
185.894559	4173.966661	6.838720	-0.037230	3.521682
186.065001	4181.942663	6.843725	-0.037267	3.524883
186.161134	4189.981538	6.848730	-0.037290	3.528103
186.469148	4198.065020	6.853734	-0.037353	3.531345
186.474550	4206.079443	6.858739	-0.037359	3.534547
186.741514	4214.139520	6.863744	-0.037415	3.537772
187.067144	4222.133784	6.868749	-0.037480	3.540969
187.280480	4230.126526	6.873754	-0.037525	3.544160
187.543573	4238.184880	6.878758	-0.037580	3.547375
187.676989	4246.200565	6.883763	-0.037610	3.550567
188.081245	4254.316773	6.888768	-0.037691	3.553803
188.438090	4262.355933	6.893773	-0.037762	3.557005
188.375268	4270.319074	6.898778	-0.037756	3.560161
188.874638	4278.334081	6.903782	-0.037854	3.563352
189.014336	4286.344070	6.908787	-0.037885	3.566527
189.166472	4294.325618	6.913792	-0.037919	3.569688
189.364835	4302.401069	6.918797	-0.037961	3.572885
189.728528	4310.410981	6.923802	-0.038034	3.576058
189.899964	4318.432545	6.928806	-0.038072	3.579227
189.803814	4326.452813	6.933811	-0.038059	3.582385
190.499650	4334.417760	6.938816	-0.038194	3.585541
190.633607	4342.485022	6.943821	-0.038224	3.588719
190.921602	4350.505605	6.948826	-0.038283	3.591880
191.221816	4358.542067	6.953830	-0.038344	3.595044
191.382560	4366.545497	6.958835	-0.038380	3.598189
191.758758	4374.560686	6.963840	-0.038455	3.601342
191.852714	4382.547965	6.968845	-0.038478	3.604473
191.983513	4390.604296	6.973850	-0.038507	3.607629
192.365198	4398.630975	6.978854	-0.038584	3.610778
192.271010	4406.693337	6.983859	-0.038572	3.613925
192.640999	4414.731109	6.988864	-0.038646	3.617072
192.998444	4422.718462	6.993869	-0.038718	3.620197
193.126944	4430.727964	6.998874	-0.038747	3.623321
193.672306	4438.750110	7.003878	-0.038854	3.626458
193.838297	4446.770291	7.008883	-0.038890	3.629582
193.991347	4454.853811	7.013888	-0.038924	3.632728
193.939471	4462.938358	7.018893	-0.038919	3.635865
194.233693	4470.878996	7.023898	-0.038979	3.638954
194.486342	4478.901070	7.028902	-0.039032	3.642070
194.563561	4486.887221	7.033907	-0.039051	3.645164
194.710232	4494.940875	7.038912	-0.039084	3.648285
194.960748	4503.003364	7.043917	-0.039136	3.651408
195.241054	4511.012652	7.048922	-0.039194	3.654509
195.371243	4519.055959	7.053926	-0.039223	3.657617
195.626734	4527.066999	7.058931	-0.039276	3.660713
195.872140	4535.103449	7.063936	-0.039327	3.663815
196.034184	4543.098835	7.068941	-0.039362	3.666897
196.186187	4551.107378	7.073946	-0.039396	3.669982
196.595703	4559.150379	7.078950	-0.039478	3.673083
196.661485	4567.178328	7.083955	-0.039495	3.676167
196.962245	4575.174792	7.088960	-0.039557	3.679243
197.258782	4583.206069	7.093965	-0.039617	3.682329
197.345853	4591.184537	7.098970	-0.039639	3.685387
197.566056	4599.266277	7.103974	-0.039685	3.688485
197.702287	4607.278695	7.108979	-0.039716	3.691552
197.844907	4615.321957	7.113984	-0.039747	3.694629
197.913963	4623.342385	7.118989	-0.039766	3.697692
198.315376	4631.305497	7.123994	-0.039846	3.700739
198.664007	4639.367264	7.128998	-0.039916	3.703820
198.923144	4647.403088	7.134003	-0.039969	3.706886
199.176727	4655.390219	7.139008	-0.040022	3.709931
199.620783	4663.482825	7.144013	-0.040110	3.713018
199.769268	4671.553437	7.149018	-0.040143	3.716087
200.018427	4679.513319	7.154022	-0.040195	3.719113
200.110061	4687.497977	7.159027	-0.040217	3.722143
200.551063	4695.459800	7.164032	-0.040304	3.725170
200.806538	4703.524085	7.169037	-0.040357	3.728229
200.965079	4711.543371	7.174042	-0.040392	3.731267
201.069726	4719.589980	7.179046	-0.040417	3.734310
201.080503	4727.640766	7.184051	-0.040424	3.737351
201.415287	4735.609362	7.189056	-0.040492	3.740365
201.704252	4743.656128	7.194061	-0.040551	3.743406
201.884045	4751.647472	7.199066	-0.040590	3.746420
202.097870	4759.698847	7.204070	-0.040635	3.749456
202.318024	4767.764766	7.209075	-0.040681	3.752495
202.583869	4775.773874	7.214080	-0.040736	3.755510
202.685982	4783.803645	7.219085	-0.040760	3.758528
202.768993	4791.822763	7.224090	-0.040781	3.761538
203.153251	4799.806849	7.229094	-0.040858	3.764540
203.227647	4807.858639	7.234099	-0.040877	3.767558
203.325944	4815.859584	7.239104	-0.040901	3.770555
203.794254	4823.912487	7.244109	-0.040993	3.773577
203.969441	4831.932678	7.249114	-0.041031	3.776578
204.017315	4839.930918	7.254118	-0.041045	3.779565
204.205935	4847.994162	7.259123	-0.041086	3.782578
204.589777	4855.958580	7.264128	-0.041163	3.785555
204.797931	4864.047093	7.269133	-0.041207	3.788572
204.884207	4872.031808	7.274138	-0.041228	3.791546
205.255886	4880.084284	7.279142	-0.041303	3.794549
205.376659	4888.126805	7.284147	-0.041330	3.797540
205.586730	4896.090641	7.289152	-0.041375	3.800502
205.847341	4904.090698	7.294157	-0.041429	3.803475
206.044680	4912.088144	7.299162	-0.041471	3.806444
206.381307	4920.158975	7.304166	-0.041539	3.809441
206.323588	4928.176172	7.309171	-0.041533	3.812407
206.711217	4936.185196	7.314176	-0.041611	3.815378
206.889051	4944.212551	7.319181	-0.041649	3.818348
206.946855	4952.229352	7.324186	-0.041665	3.821309
207.538060	4960.237561	7.329190	-0.041781	3.824277
207.660674	4968.255715	7.334195	-0.041809	3.827235
207.689864	4976.285368	7.339200	-0.041819	3.830194
207.909925	4984.358959	7.344205	-0.041866	3.833171
208.126079	4992.347443	7.349210	-0.041911	3.836113
208.581881	5000.347578	7.354214	-0.042001	3.839063
208.661478	5008.395254	7.359219	-0.042022	3.842020
208.994886	5016.349249	7.364224	-0.042089	3.844946
209.325856	5024.427128	7.369229	-0.042156	3.847915
209.387825	5032.428917	7.374234	-0.042173	3.850848
209.806171	5040.483130	7.379238	-0.042256	3.853805
210.077155	5048.520976	7.384243	-0.042312	3.856751
210.291224	5056.517761	7.389248	-0.042357	3.859678
210.506014	5064.570270	7.394253	-0.042402	3.862624
210.662625	5072.523476	7.399258	-0.042437	3.865530
210.933551	5080.593093	7.404262	-0.042492	3.868478
210.975835	5088.650314	7.409267	-0.042506	3.871415
211.278072	5096.883429	7.414272	-0.042567	3.874419
211.470625	5104.867083	7.419277	-0.042609	3.877328
211.614698	5112.704763	7.424282	-0.042641	3.880181
211.999042	5120.742836	7.429286	-0.042717	3.883109
212.036466	5128.714094	7.434291	-0.042730	3.886003
212.350865	5136.750934	7.439296	-0.042794	3.888925
212.674934	5144.794322	7.444301	-0.042859	3.891847
212.842483	5152.848542	7.449306	-0.042896	3.894767
212.964444	5160.858599	7.454310	-0.042924	3.897669
213.143052	5168.807018	7.459315	-0.042962	3.900547
213.422516	5176.817593	7.464320	-0.043020	3.903447
213.723198	5184.866037	7.469325	-0.043081	3.906360
213.850184	5192.877501	7.474330	-0.043110	3.909253
214.164707	5200.931397	7.479334	-0.043174	3.912163
214.115190	5208.951672	7.484339	-0.043170	3.915052
214.458683	5216.932145	7.489344	-0.043239	3.917932
214.538386	5224.942225	7.494349	-0.043259	3.920815
214.820335	5232.923867	7.499354	-0.043317	3.923690
215.115419	5240.992556	7.504358	-0.043377	3.926594
215.137990	5248.985967	7.509363	-0.043387	3.929464
215.414260	5257.055484	7.514368	-0.043444	3.932364
215.659374	5265.082075	7.519373	-0.043495	3.935246
215.750439	5273.079447	7.524378	-0.043517	3.938112
216.082647	5281.080586	7.529382	-0.043584	3.940982
216.254897	5289.064004	7.534387	-0.043621	3.943840
216.353281	5297.111027	7.539392	-0.043645	3.946718
216.491364	5305.170814	7.544397	-0.043676	3.949599
216.749801	5313.178301	7.549402	-0.043729	3.952461
217.104051	5321.244078	7.554406	-0.043801	3.955344
217.030026	5329.223125	7.559411	-0.043792	3.958186
217.322903	5337.203737	7.564416	-0.043852	3.961033
217.664943	5345.217753	7.569421	-0.043921	3.963891
217.837564	5353.199958	7.574426	-0.043958	3.966732
218.027447	5361.265386	7.579430	-0.043999	3.969601
218.001144	5369.315099	7.584435	-0.044000	3.972459
218.302174	5377.361652	7.589440	-0.044061	3.975319
218.628292	5385.388321	7.594445	-0.044127	3.978170
218.796573	5393.353195	7.599450	-0.044164	3.980995
219.028091	5401.372084	7.604454	-0.044212	3.983838
219.020871	5409.396166	7.609459	-0.044216	3.986677
219.253926	5417.439849	7.614464	-0.044265	3.989525
219.573898	5425.486359	7.619469	-0.044330	3.992372
219.619752	5433.519191	7.624474	-0.044343	3.995209
220.055281	5441.558971	7.629478	-0.044430	3.998052
220.254369	5449.516829	7.634483	-0.044472	4.000861
220.619032	5457.496988	7.639488	-0.044545	4.003678
220.634017	5465.554209	7.644493	-0.044553	4.006514
220.948353	5473.564088	7.649498	-0.044617	4.009337
221.361129	5481.600335	7.654502	-0.044699	4.012168
221.122315	5489.654729	7.659507	-0.044660	4.014994
221.216571	5497.683404	7.664512	-0.044683	4.017814
221.677081	5505.689544	7.669517	-0.044774	4.020629
221.820118	5513.666093	7.674522	-0.044806	4.023428
221.955553	5521.726153	7.679526	-0.044837	4.026253
222.121109	5529.721071	7.684531	-0.044873	4.029054
222.288109	5537.759960	7.689536	-0.044909	4.031869
222.498198	5545.905480	7.694541	-0.044954	4.034719
222.814313	5553.841416	7.699546	-0.045018	4.037496
223.128873	5561.817019	7.704550	-0.045082	4.040284
223.103797	5569.823094	7.709555	-0.045082	4.043077
223.406474	5577.803260	7.714560	-0.045144	4.045863
223.598505	5585.853675	7.719565	-0.045185	4.048670
223.632179	5593.863301	7.724570	-0.045197	4.051458
223.821629	5601.917922	7.729574	-0.045237	4.054263
224.008579	5609.915417	7.734579	-0.045277	4.057045
224.459200	5617.902475	7.739584	-0.045367	4.059826
224.624712	5625.962414	7.744589	-0.045403	4.062626
224.822741	5633.915955	7.749594	-0.045445	4.065388
225.249990	5641.993832	7.754598	-0.045530	4.068194
225.257528	5649.993070	7.759603	-0.045536	4.070965
225.476821	5658.016516	7.764608	-0.045583	4.073746
225.661722	5666.053206	7.769613	-0.045622	4.076528
225.884546	5674.033469	7.774618	-0.045669	4.079290
226.196411	5682.090830	7.779622	-0.045732	4.082078
226.364144	5690.039971	7.784627	-0.045769	4.084824
226.430764	5698.105236	7.789632	-0.045787	4.087607
226.719209	5706.109602	7.794637	-0.045846	4.090371
226.770653	5714.132120	7.799642	-0.045861	4.093135
227.169381	5722.155157	7.804646	-0.045940	4.095902
227.329799	5730.158241	7.809651	-0.045975	4.098658
227.409223	5738.180709	7.814656	-0.045995	4.101417
227.500136	5746.229101	7.819661	-0.046018	4.104184
227.596943	5754.239999	7.824666	-0.046041	4.106935
227.783777	5762.285779	7.829670	-0.046081	4.109698
228.112796	5770.307271	7.834675	-0.046148	4.112453
228.363787	5778.338945	7.839680	-0.046200	4.115208
228.422732	5786.411330	7.844685	-0.046216	4.117973
228.502836	5794.336907	7.849690	-0.046236	4.120686
228.731590	5802.389379	7.854694	-0.046284	4.123442
228.846926	5810.353588	7.859699	-0.046311	4.126165
229.171196	5818.414492	7.864704	-0.046377	4.128922
229.475474	5826.423977	7.869709	-0.046439	4.131659
229.727561	5834.434322	7.874714	-0.046491	4.134394
229.738832	5842.527183	7.879718	-0.046498	4.137152
230.075870	5850.510578	7.884723	-0.046566	4.139875
230.173633	5858.547974	7.889728	-0.046590	4.142612
230.269822	5866.496216	7.894733	-0.046613	4.145317
230.162838	5874.550316	7.899738	-0.046598	4.148053
230.535647	5882.598084	7.904742	-0.046673	4.150791
230.780554	5890.646424	7.909747	-0.046724	4.153526
230.936532	5898.608325	7.914752	-0.046758	4.156229
231.080947	5906.647719	7.919757	-0.046791	4.158956
231.280643	5914.649151	7.924762	-0.046833	4.161669
231.723030	5922.668226	7.929766	-0.046921	4.164389
231.657252	5930.678845	7.934771	-0.046914	4.167098
232.046774	5938.652192	7.939776	-0.046992	4.169798
232.026188	5946.730043	7.944781	-0.046993	4.172528
231.937282	5954.761728	7.949786	-0.046982	4.175239
232.283190	5962.778289	7.954790	-0.047052	4.177948
232.426400	5970.742715	7.959795	-0.047084	4.180635
232.652954	5978.780140	7.964800	-0.047131	4.183346
232.843635	5986.797109	7.969805	-0.047172	4.186048
233.166161	5994.794840	7.974810	-0.047237	4.188744
233.410575	6002.879193	7.979814	-0.047288	4.191465
233.525023	6010.977538	7.984819	-0.047315	4.194189
233.719811	6018.936512	7.989824	-0.047356	4.196864
234.149326	6026.905645	7.994829	-0.047442	4.199544
234.116070	6034.906062	7.999834	-0.047441	4.202228
234.499690	6042.903798	8.004838	-0.047517	4.204913
234.677473	6050.893342	8.009843	-0.047556	4.207591
234.765575	6058.884173	8.014848	-0.047577	4.210268
235.033539	6067.013929	8.019853	-0.047633	4.212991
235.229952	6074.980239	8.024858	-0.047675	4.215657
235.147179	6083.033567	8.029862	-0.047664	4.218347
235.401885	6090.999108	8.034867	-0.047717	4.221010
235.685300	6099.026050	8.039872	-0.047775	4.223692
235.692565	6107.058539	8.044877	-0.047782	4.226371
235.747013	6115.038597	8.049882	-0.047797	4.229032
236.229510	6123.102706	8.054886	-0.047892	4.231723
236.498094	6131.122732	8.059891	-0.047948	4.234395
236.344859	6139.210232	8.064896	-0.047925	4.237084
236.545895	6147.180428	8.069901	-0.047967	4.239736
236.662062	6155.169283	8.074906	-0.047994	4.242392
237.059012	6163.123667	8.079910	-0.048073	4.245037
236.951141	6171.191715	8.084915	-0.048059	4.247713
237.141688	6179.194752	8.089920	-0.048099	4.250369
237.411653	6187.239422	8.094925	-0.048155	4.253038
237.494119	6195.261162	8.099930	-0.048176	4.255696
237.778934	6203.307241	8.104934	-0.048234	4.258361
237.871050	6211.258658	8.109939	-0.048256	4.260993
238.123425	6219.329019	8.114944	-0.048309	4.263663
238.549747	6227.327362	8.119949	-0.048394	4.266309
238.696490	6235.337882	8.124954	-0.048426	4.268955
238.993298	6243.378088	8.129958	-0.048487	4.271611
238.982534	6251.464184	8.134963	-0.048490	4.274277
239.441174	6259.495482	8.139968	-0.048581	4.276928
239.813964	6267.443969	8.144973	-0.048655	4.279549
239.681627	6275.459028	8.149978	-0.048636	4.282186
239.774320	6283.432766	8.154982	-0.048659	4.284810
240.093043	6291.499160	8.159987	-0.048723	4.287464
240.221861	6299.436387	8.164992	-0.048753	4.290073
240.394727	6307.558191	8.169997	-0.048790	4.292741
240.515046	6315.535971	8.175002	-0.048818	4.295360
240.841404	6323.629171	8.180006	-0.048884	4.298016
240.991267	6331.579076	8.185011	-0.048917	4.300623
240.891869	6339.629129	8.190016	-0.048904	4.303259
241.290963	6347.622359	8.195021	-0.048984	4.305878
241.435310	6355.613869	8.200026	-0.049016	4.308493
241.722640	6363.659694	8.205030	-0.049075	4.311126
241.827348	6371.696382	8.210035	-0.049099	4.313752
241.968334	6379.720019	8.215040	-0.049131	4.316373
242.241156	6387.704624	8.220045	-0.049187	4.318981
242.551908	6395.682835	8.225050	-0.049250	4.321585
242.764649	6403.707336	8.230054	-0.049295	4.324202
242.643050	6411.738000	8.235059	-0.049278	4.326817
242.752484	6419.741855	8.240064	-0.049303	4.329423
243.067354	6427.846220	8.245069	-0.049367	4.332062
243.166384	6435.790979	8.250074	-0.049391	4.334645
243.331699	6443.854529	8.255078	-0.049427	4.337267
243.464600	6451.792887	8.260083	-0.049457	4.339845
243.891525	6459.836100	8.265088	-0.049542	4.342459
244.003113	6467.830774	8.270093	-0.049568	4.345052
244.293794	6475.862478	8.275098	-0.049628	4.347658
244.528771	6483.888618	8.280102	-0.049677	4.350259
244.690986	6491.917178	8.285107	-0.049712	4.352859
244.863104	6500.020886	8.290112	-0.049750	4.355483
245.355822	6508.046380	8.295117	-0.049847	4.358081
245.323846	6515.957927	8.300122	-0.049846	4.360637
245.363227	6524.006257	8.305126	-0.049859	4.363237
245.514204	6531.959699	8.310131	-0.049892	4.365805
245.833764	6540.003976	8.315136	-0.049957	4.368402
246.173284	6548.004395	8.320141	-0.050025	4.370983
246.364674	6556.043262	8.325146	-0.050066	4.373575
246.565295	6564.094583	8.330150	-0.050109	4.376168
246.604964	6572.098176	8.335155	-0.050122	4.378744
246.556305	6580.090502	8.340160	-0.050118	4.381315
246.821662	6588.096904	8.345165	-0.050172	4.383890
247.000831	6596.087173	8.350170	-0.050211	4.386458
247.250256	6604.139434	8.355174	-0.050263	4.389044
247.564510	6612.165352	8.360179	-0.050327	4.391621
247.668836	6620.183834	8.365184	-0.050351	4.394193
247.837609	6628.262580	8.370189	-0.050388	4.396783
247.864587	6636.194288	8.375194	-0.050399	4.399324
248.253005	6644.228544	8.380198	-0.050476	4.401897
248.481815	6652.220266	8.385203	-0.050524	4.404455
248.469213	6660.247635	8.390208	-0.050527	4.407022
248.809259	6668.292154	8.395213	-0.050596	4.409594
249.016512	6676.282791	8.400218	-0.050640	4.412147
249.176529	6684.362960	8.405222	-0.050675	4.414727
249.163986	6692.388654	8.410227	-0.050678	4.417287
249.536335	6700.320659	8.415232	-0.050752	4.419817
249.881160	6708.437106	8.420237	-0.050822	4.422405
249.796725	6716.373921	8.425242	-0.050811	4.424932
250.281185	6724.423557	8.430246	-0.050907	4.427495
250.396255	6732.456336	8.435251	-0.050934	4.430051
250.575556	6740.476287	8.440256	-0.050972	4.432601
250.808088	6748.512063	8.445261	-0.051021	4.435155
250.932371	6756.517517	8.450266	-0.051049	4.437697
251.156796	6764.519512	8.455270	-0.051096	4.440237
251.375792	6772.538068	8.460275	-0.051143	4.442781
251.493344	6780.505362	8.465280	-0.051170	4.445306
251.691964	6788.567003	8.470285	-0.051212	4.447861
251.731315	6796.526671	8.475290	-0.051225	4.450381
252.025026	6804.628182	8.480294	-0.051285	4.452945
252.110650	6812.608391	8.485299	-0.051306	4.455469
252.243129	6820.622306	8.490304	-0.051336	4.458002
252.642968	6828.612301	8.495309	-0.051416	4.460527
252.805637	6836.660898	8.500314	-0.051451	4.463069
253.331016	6844.658984	8.505318	-0.051554	4.465594
253.156712	6852.695555	8.510323	-0.051527	4.468127
253.422167	6860.711503	8.515328	-0.051582	4.470654
253.737673	6868.761365	8.520333	-0.051646	4.473191
253.617993	6876.737682	8.525338	-0.051629	4.475701
253.935880	6884.766022	8.530342	-0.051693	4.478228
254.043208	6892.750276	8.535347	-0.051719	4.480738
254.359920	6900.770005	8.540352	-0.051783	4.483259
254.698577	6908.762374	8.545357	-0.051851	4.485770
254.955604	6916.790894	8.550362	-0.051905	4.488291
254.959510	6924.840059	8.555366	-0.051911	4.490816
255.100466	6932.879713	8.560371	-0.051942	4.493337
255.552685	6940.881642	8.565376	-0.052032	4.495846
255.609596	6948.899227	8.570381	-0.052048	4.498357
255.805572	6956.900331	8.575386	-0.052089	4.500861
255.842655	6964.939076	8.580391	-0.052102	4.503376
255.991578	6972.880664	8.585395	-0.052135	4.505859
256.089758	6980.925988	8.590400	-0.052158	4.508374
256.191612	6988.924828	8.595405	-0.052182	4.510872
256.530216	6997.029674	8.600410	-0.052251	4.513402
256.703034	7005.023123	8.605415	-0.052288	4.515896
256.841049	7013.042312	8.610419	-0.052319	4.518396
257.115932	7020.999055	8.615424	-0.052376	4.520876
257.339849	7029.048817	8.620429	-0.052423	4.523384
257.436194	7036.997487	8.625434	-0.052446	4.525858
257.666548	7045.064288	8.630439	-0.052494	4.528368
257.799045	7053.050784	8.635443	-0.052524	4.530851
257.861621	7061.096333	8.640448	-0.052541	4.533351
258.084461	7069.176777	8.645453	-0.052588	4.535861
258.291771	7077.136096	8.650458	-0.052632	4.538331
258.545191	7085.139911	8.655463	-0.052684	4.540815
258.566367	7093.157228	8.660467	-0.052694	4.543300
258.919422	7101.145404	8.665472	-0.052765	4.545776
259.025422	7109.224709	8.670477	-0.052790	4.548278
259.022522	7117.174712	8.675482	-0.052794	4.550739
259.515704	7125.269711	8.680487	-0.052892	4.553244
259.638751	7133.261445	8.685491	-0.052920	4.555715
259.835333	7141.254327	8.690496	-0.052962	4.558185
260.131395	7149.275625	8.695501	-0.053022	4.560663
260.188384	7157.308086	8.700506	-0.053038	4.563142
260.397185	7165.320298	8.705511	-0.053082	4.565614
260.406128	7173.337370	8.710515	-0.053089	4.568086
260.652827	7181.285374	8.715520	-0.053140	4.570536
261.069268	7189.367227	8.720525	-0.053223	4.573025
261.069153	7197.337641	8.725530	-0.053229	4.575479
261.390194	7205.437767	8.730535	-0.053294	4.577971
261.380853	7213.379318	8.735539	-0.053297	4.580413
261.538048	7221.449933	8.740544	-0.053332	4.582894
261.768464	7229.401918	8.745549	-0.053380	4.585336
262.093044	7237.441599	8.750554	-0.053446	4.587805
262.518012	7245.444998	8.755559	-0.053530	4.590260
262.578127	7253.520130	8.760563	-0.053547	4.592737
262.651434	7261.531389	8.765568	-0.053566	4.595192
262.949296	7269.607164	8.770573	-0.053626	4.597666
262.826638	7277.513844	8.775578	-0.053609	4.600087
263.247946	7285.597449	8.780583	-0.053693	4.602560
263.375720	7293.526051	8.785587	-0.053722	4.604985
263.552205	7301.579489	8.790592	-0.053760	4.607447
263.646778	7309.585083	8.795597	-0.053783	4.609893
263.551977	7317.646866	8.800602	-0.053770	4.612354
263.925853	7325.666606	8.805607	-0.053845	4.614802
264.064775	7333.703645	8.810611	-0.053877	4.617253
264.139989	7341.618897	8.815616	-0.053896	4.619666
264.485132	7349.696747	8.820621	-0.053965	4.622127
264.700931	7357.655684	8.825626	-0.054011	4.624551
264.980370	7365.748328	8.830631	-0.054068	4.627014
265.098101	7373.761802	8.835635	-0.054096	4.629451
265.319732	7381.745969	8.840640	-0.054142	4.631879
265.514478	7389.821683	8.845645	-0.054184	4.634333
265.522789	7397.802428	8.850650	-0.054190	4.636757
265.977366	7405.804381	8.855655	-0.054280	4.639185
266.029070	7413.782438	8.860659	-0.054295	4.641606
266.140014	7421.774189	8.865664	-0.054321	4.644029
266.328514	7429.823036	8.870669	-0.054362	4.646468
266.793074	7437.861931	8.875674	-0.054454	4.648903
266.769232	7445.889601	8.880679	-0.054454	4.651333
266.979192	7453.892650	8.885683	-0.054499	4.653755
267.239762	7461.904337	8.890688	-0.054553	4.656177
267.366644	7469.938215	8.895693	-0.054582	4.658606
267.409076	7477.923177	8.900698	-0.054595	4.661018
267.715230	7485.935476	8.905703	-0.054657	4.663437
267.776092	7493.939276	8.910707	-0.054674	4.665852
267.960410	7501.985255	8.915712	-0.054713	4.668279
268.285655	7510.014612	8.920717	-0.054779	4.670699
268.444629	7518.033746	8.925722	-0.054814	4.673115
268.567423	7526.120115	8.930727	-0.054842	4.675551
268.838398	7534.093483	8.935731	-0.054898	4.677950
268.968187	7542.045172	8.940736	-0.054927	4.680342
269.122538	7550.067626	8.945741	-0.054962	4.682754
269.301487	7558.038355	8.950746	-0.055000	4.685150
269.652563	7566.127846	8.955751	-0.055071	4.687579
269.681664	7574.089185	8.960755	-0.055082	4.689969
269.630055	7582.138261	8.965760	-0.055077	4.692384
270.111159	7590.181204	8.970765	-0.055172	4.694796
270.431710	7598.159433	8.975770	-0.055237	4.697186
270.358551	7606.160410	8.980775	-0.055229	4.699584
270.338387	7614.200324	8.985779	-0.055230	4.701991
270.709985	7622.129936	8.990784	-0.055305	4.704364
270.767795	7630.242493	8.995789	-0.055321	4.706791
270.865537	7638.188352	9.000794	-0.055344	4.709166
271.024260	7646.264241	9.005799	-0.055379	4.711579
271.332457	7654.291417	9.010803	-0.055442	4.713976
271.458103	7662.304271	9.015808	-0.055471	4.716368
271.706592	7670.324578	9.020813	-0.055522	4.718760
271.912152	7678.311970	9.025818	-0.055566	4.721142
271.939710	7686.347719	9.030823	-0.055576	4.723537
272.063558	7694.335134	9.035827	-0.055605	4.725916
272.151111	7702.377624	9.040832	-0.055626	4.728311
272.484494	7710.365040	9.045837	-0.055694	4.730687
272.514464	7718.377346	9.050842	-0.055705	4.733070
272.872439	7726.426867	9.055847	-0.055776	4.735462
273.043021	7734.475274	9.060851	-0.055814	4.737853
273.303945	7742.445830	9.065856	-0.055867	4.740220
273.564768	7750.535137	9.070861	-0.055921	4.742620
273.715220	7758.376818	9.075866	-0.055955	4.744947
273.983580	7766.513446	9.080871	-0.056010	4.747359
274.054177	7774.505390	9.085875	-0.056028	4.749727
274.405367	7782.547115	9.090880	-0.056099	4.752108
274.627252	7790.660940	9.095885	-0.056146	4.754510
274.717098	7798.565138	9.100890	-0.056168	4.756849
275.102218	7806.598624	9.105895	-0.056245	4.759224
275.411078	7814.623625	9.110899	-0.056308	4.761596
275.432194	7822.568475	9.115904	-0.056317	4.763943
275.704337	7830.574690	9.120909	-0.056373	4.766307
276.079249	7838.605491	9.125914	-0.056448	4.768676
276.215188	7846.626419	9.130919	-0.056478	4.771042
276.288024	7854.682235	9.135923	-0.056497	4.773418
276.511608	7862.692418	9.140928	-0.056544	4.775778
276.821860	7870.716435	9.145933	-0.056607	4.778141
276.913493	7878.671246	9.150938	-0.056630	4.780483
277.322144	7886.755823	9.155943	-0.056711	4.782861
277.229338	7894.704097	9.160947	-0.056699	4.785199
277.217457	7902.749903	9.165952	-0.056702	4.787565
277.639495	7910.774740	9.170957	-0.056786	4.789922
277.930754	7918.805839	9.175962	-0.056846	4.792280
278.120543	7926.845736	9.180967	-0.056886	4.794639
278.207615	7934.861372	9.185971	-0.056908	4.796991
278.484448	7942.770241	9.190976	-0.056965	4.799309
278.648990	7950.875011	9.195981	-0.057001	4.801685
278.583561	7958.778504	9.200986	-0.056994	4.804001
278.803833	7966.851746	9.205991	-0.057040	4.806364
278.867706	7974.863375	9.210995	-0.057057	4.808709
278.985809	7982.890581	9.216000	-0.057085	4.811057
279.347321	7990.363392	9.221005	-0.057157	4.813241
279.543839	7994.908863	9.226010	-0.057196	4.814568

279.702524	7997.224309	9.231015	-0.057228	4.815244
279.782148	7998.580345	9.236019	-0.057243	4.815640
279.850990	7999.116843	9.241024	-0.057257	4.815797
279.987813	7999.901397	9.246029	-0.057283	4.816025
280.010342	7999.852667	9.251034	-0.057287	4.816011
280.247960	7999.878355	9.256039	-0.057331	4.816017
280.416711	7999.879288	9.261043	-0.057363	4.816016
280.207437	7999.853061	9.266048	-0.057324	4.816010
280.342686	7999.897192	9.271053	-0.057349	4.816022
280.388081	7999.902298	9.276058	-0.057358	4.816023
280.532382	7999.822655	9.281063	-0.057385	4.815999
280.506874	7999.883101	9.286067	-0.057380	4.816017
280.707057	7999.870716	9.291072	-0.057417	4.816012
280.943703	7999.934852	9.296077	-0.057461	4.816030
280.676676	7999.896891	9.301082	-0.057412	4.816020
280.792341	7999.959900	9.306087	-0.057433	4.816038
280.893968	7999.879482	9.311091	-0.057452	4.816014
280.921445	7999.899221	9.316096	-0.057458	4.816020
280.952397	7999.928639	9.321101	-0.057464	4.816028
281.045436	7999.891871	9.326106	-0.057481	4.816017
281.211478	7999.873525	9.331111	-0.057512	4.816010
281.088518	7999.947160	9.336115	-0.057489	4.816033
281.174434	7999.849362	9.341120	-0.057505	4.816004
281.296679	7999.948819	9.346125	-0.057528	4.816032
281.133249	7999.915943	9.351130	-0.057498	4.816023
281.119080	7999.932788	9.356135	-0.057495	4.816028
281.351852	7999.935954	9.361139	-0.057539	4.816028
281.358131	7999.911501	9.366144	-0.057540	4.816021
281.406149	7999.952983	9.371149	-0.057549	4.816033
281.314655	7999.936371	9.376154	-0.057532	4.816028
281.687871	7999.918581	9.381159	-0.057601	4.816021
281.536573	7999.922252	9.386163	-0.057573	4.816023
281.517217	7999.879170	9.391168	-0.057570	4.816010
281.578023	7999.927294	9.396173	-0.057581	4.816024
281.410139	7999.879379	9.401178	-0.057550	4.816011
281.566432	7999.921757	9.406183	-0.057579	4.816023
281.742802	7999.946337	9.411187	-0.057612	4.816029
281.714176	7999.872101	9.416192	-0.057607	4.816007
281.607046	7999.906492	9.421197	-0.057587	4.816018
281.485609	7999.889336	9.426202	-0.057564	4.816014
281.585534	7999.943513	9.431207	-0.057583	4.816029
281.611027	7999.961079	9.436211	-0.057588	4.816034
281.748645	7999.867424	9.441216	-0.057614	4.816006
281.601576	7999.957718	9.446221	-0.057586	4.816033
281.748730	7999.894153	9.451226	-0.057614	4.816014
281.814124	7999.911376	9.456231	-0.057626	4.816018
281.860185	7999.950685	9.461235	-0.057635	4.816030
281.919067	7999.912229	9.466240	-0.057646	4.816018
281.890097	7999.973682	9.471245	-0.057641	4.816036
281.880313	7999.905130	9.476250	-0.057639	4.816016
282.052631	7999.920020	9.481255	-0.057671	4.816020
282.048794	7999.933849	9.486259	-0.057670	4.816024
281.965081	7999.872502	9.491264	-0.057655	4.816006
282.069496	7999.953473	9.496269	-0.057674	4.816029
281.997185	7999.890196	9.501274	-0.057661	4.816011
282.004228	7999.932002	9.506279	-0.057662	4.816023
282.005650	7999.940584	9.511283	-0.057663	4.816026
282.236318	7999.848618	9.516288	-0.057706	4.815998
282.209650	7999.971017	9.521293	-0.057701	4.816034
282.014192	7999.941831	9.526298	-0.057665	4.816026
282.097763	7999.975411	9.531303	-0.057680	4.816035
282.104518	7999.949898	9.536307	-0.057682	4.816028
282.082426	7999.924930	9.541312	-0.057677	4.816021
282.122828	7999.994054	9.546317	-0.057685	4.816041
282.155644	7999.895290	9.551322	-0.057691	4.816012
282.170329	7999.924413	9.556327	-0.057694	4.816020
282.103213	7999.941366	9.561331	-0.057682	4.816025
282.189815	7999.872428	9.566336	-0.057698	4.816005
282.022343	7999.961283	9.571341	-0.057667	4.816032
282.113705	7999.924485	9.576346	-0.057684	4.816020
282.067374	7999.938610	9.581351	-0.057675	4.816025
282.261977	7999.918646	9.586355	-0.057712	4.816018
282.375142	7999.910024	9.591360	-0.057733	4.816015
282.502682	7999.978595	9.596365	-0.057757	4.816034
282.282780	7999.912636	9.601370	-0.057716	4.816016
282.170414	7999.923425	9.606375	-0.057695	4.816020
282.192303	7999.945200	9.611379	-0.057699	4.816026
282.325288	7999.910227	9.616384	-0.057724	4.816015
282.363819	7999.937647	9.621389	-0.057731	4.816023
282.153377	7999.915668	9.626394	-0.057692	4.816018
282.328606	7999.929543	9.631399	-0.057725	4.816021
282.253922	7999.930332	9.636403	-0.057711	4.816021
282.390332	7999.867640	9.641408	-0.057736	4.816002
282.398632	7999.864593	9.646413	-0.057738	4.816001
282.278654	7999.886997	9.651418	-0.057716	4.816009
282.349976	7999.947067	9.656423	-0.057729	4.816026
282.473598	7999.997402	9.661427	-0.057752	4.816040
282.317753	7999.937949	9.666432	-0.057723	4.816023
282.521694	8000.004703	9.671437	-0.057761	4.816042
282.352770	7999.917232	9.676442	-0.057730	4.816017
282.529990	7999.961061	9.681447	-0.057763	4.816029
282.568716	7999.962841	9.686451	-0.057770	4.816029
282.345190	7999.958788	9.691456	-0.057729	4.816029
282.572524	7999.981090	9.696461	-0.057771	4.816035
282.644965	7999.946085	9.701466	-0.057785	4.816024
282.579192	7999.960926	9.706471	-0.057773	4.816029
282.417457	7999.952653	9.711475	-0.057743	4.816027
282.692084	7999.928801	9.716480	-0.057794	4.816019
282.820676	7999.958925	9.721485	-0.057818	4.816027
282.586563	7999.918352	9.726490	-0.057774	4.816016
282.540924	7999.899366	9.731495	-0.057766	4.816011
282.626706	7999.937261	9.736499	-0.057782	4.816021
282.438707	7999.895388	9.741504	-0.057747	4.816010
282.609610	8000.000007	9.746509	-0.057779	4.816040
282.480251	7999.941035	9.751514	-0.057755	4.816023
282.541655	7999.922926	9.756519	-0.057766	4.816018
282.680561	7999.888060	9.761523	-0.057792	4.816007
282.809945	7999.848747	9.766528	-0.057817	4.815995
282.749876	7999.970540	9.771533	-0.057806	4.816030
282.606909	7999.959403	9.776538	-0.057779	4.816028
282.968640	7999.967051	9.781543	-0.057846	4.816028
282.977958	7999.957612	9.786547	-0.057848	4.816025
282.942203	7999.989025	9.791552	-0.057842	4.816035
282.882377	7999.996494	9.796557	-0.057831	4.816037
282.774700	7999.947532	9.801562	-0.057811	4.816024
282.758192	7999.914116	9.806567	-0.057808	4.816014
282.803261	7999.914943	9.811571	-0.057816	4.816014
282.787629	7999.930694	9.816576	-0.057813	4.816019
282.980454	7999.954507	9.821581	-0.057849	4.816025
282.911298	7999.917998	9.826586	-0.057836	4.816014
282.841375	7999.898571	9.831591	-0.057823	4.816009
282.832805	7999.962533	9.836595	-0.057822	4.816028
282.786956	7999.928585	9.841600	-0.057814	4.816018
282.907861	7999.969255	9.846605	-0.057836	4.816029
282.780477	7999.899633	9.851610	-0.057812	4.816010
282.817238	7999.901377	9.856615	-0.057819	4.816010
282.769189	7999.957143	9.861619	-0.057811	4.816026
282.906164	7999.912625	9.866624	-0.057836	4.816013
282.890251	7999.963632	9.871629	-0.057833	4.816028
282.729047	7999.953232	9.876634	-0.057803	4.816025
282.723291	7999.946724	9.881639	-0.057802	4.816024
282.974116	7999.964111	9.886643	-0.057849	4.816027
282.727699	7999.951094	9.891648	-0.057803	4.816025
282.832118	8000.008561	9.896653	-0.057823	4.816041
282.796905	7999.937408	9.901658	-0.057816	4.816020
283.060676	7999.983880	9.906663	-0.057866	4.816033
282.741757	7999.981299	9.911667	-0.057806	4.816034
282.750824	7999.953690	9.916672	-0.057808	4.816025
282.986268	7999.986825	9.921677	-0.057852	4.816034
282.915619	7999.935330	9.926682	-0.057839	4.816019
282.766485	7999.942245	9.931687	-0.057811	4.816022
283.011180	7999.974480	9.936691	-0.057857	4.816030
283.111673	7999.978451	9.941696	-0.057876	4.816031
283.219925	8000.041331	9.946701	-0.057896	4.816049
283.084375	7999.969422	9.951706	-0.057871	4.816028
283.123000	7999.985091	9.956711	-0.057878	4.816033
282.943639	8000.005347	9.961715	-0.057845	4.816040
282.844353	7999.946921	9.966720	-0.057826	4.816023
283.016562	7999.932961	9.971725	-0.057858	4.816018
282.940737	7999.885646	9.976730	-0.057844	4.816005
283.067928	7999.911472	9.981735	-0.057868	4.816011
283.079915	7999.992904	9.986739	-0.057870	4.816035
282.931189	7999.973113	9.991744	-0.057843	4.816030
283.037270	8000.019926	9.996749	-0.057863	4.816043
283.061254	7999.937026	10.001754	-0.057867	4.816019
282.999399	7999.955143	10.006759	-0.057856	4.816025
282.981144	7999.986874	10.011763	-0.057852	4.816034
282.912605	7999.961062	10.016768	-0.057840	4.816027
283.052169	7999.992455	10.021773	-0.057866	4.816035
282.934924	7999.923017	10.026778	-0.057844	4.816015
283.019609	7999.899988	10.031783	-0.057860	4.816008
282.983158	7999.958101	10.036787	-0.057853	4.816025
283.010080	7999.874187	10.041792	-0.057858	4.816001
283.137149	7999.935271	10.046797	-0.057882	4.816018
283.036527	7999.891779	10.051802	-0.057863	4.816006
283.116901	7999.887904	10.056807	-0.057878	4.816004
283.196498	7999.941715	10.061811	-0.057893	4.816020
283.136997	7999.990862	10.066816	-0.057882	4.816034
283.205022	8000.019887	10.071821	-0.057895	4.816042
283.045937	7999.965716	10.076826	-0.057866	4.816027
283.080834	7999.938577	10.081831	-0.057872	4.816019
283.231685	8000.001162	10.086835	-0.057900	4.816037
283.241370	7999.924413	10.091840	-0.057902	4.816014
283.297475	8000.005579	10.096845	-0.057913	4.816038
283.360747	8000.007805	10.101850	-0.057925	4.816038
283.304851	7999.985427	10.106855	-0.057914	4.816032
283.475563	7999.987469	10.111859	-0.057946	4.816031
283.333063	7999.917571	10.116864	-0.057920	4.816012
283.188098	7999.968370	10.121869	-0.057893	4.816027
283.158462	7999.988141	10.126874	-0.057887	4.816033
283.156583	7999.989183	10.131879	-0.057887	4.816034
283.274808	8000.016984	10.136883	-0.057909	4.816041
283.125224	7999.942683	10.141888	-0.057881	4.816020
283.151727	7999.985913	10.146893	-0.057886	4.816033
282.977174	7999.919708	10.151898	-0.057854	4.816014
283.150042	7999.904692	10.156903	-0.057886	4.816009
283.318557	7999.965461	10.161907	-0.057918	4.816026
283.080575	7999.877802	10.166912	-0.057873	4.816001
283.346152	7999.856991	10.171917	-0.057923	4.815994
283.324869	7999.930339	10.176922	-0.057919	4.816015
283.279099	7999.911350	10.181927	-0.057911	4.816010
283.362588	7999.945999	10.186931	-0.057926	4.816020
283.300688	7999.902142	10.191936	-0.057915	4.816007
283.371112	7999.949375	10.196941	-0.057928	4.816021
283.094639	7999.982826	10.201946	-0.057877	4.816032
283.251796	7999.980347	10.206951	-0.057906	4.816030
283.319537	7999.985860	10.211955	-0.057919	4.816032
283.300880	7999.892568	10.216960	-0.057915	4.816005
283.241586	7999.965226	10.221965	-0.057904	4.816026
283.314622	7999.962287	10.226970	-0.057918	4.816025
283.206283	7999.937887	10.231975	-0.057898	4.816018
283.269503	7999.970031	10.236979	-0.057910	4.816027
283.327460	7999.926214	10.241984	-0.057921	4.816014
283.503524	7999.948655	10.246989	-0.057954	4.816020
283.216004	7999.957329	10.251994	-0.057900	4.816024
283.367757	7999.941929	10.256999	-0.057928	4.816019
283.409791	7999.964071	10.262003	-0.057936	4.816025
283.287268	7999.830427	10.267008	-0.057913	4.815986
283.505393	7999.939112	10.272013	-0.057954	4.816017
283.453897	7999.886895	10.277018	-0.057945	4.816002
283.311888	7999.886460	10.282023	-0.057918	4.816003
283.267544	7999.954047	10.287027	-0.057910	4.816023
283.368599	7999.924904	10.292032	-0.057929	4.816014
283.395832	7999.976695	10.297037	-0.057934	4.816029
283.379825	7999.942220	10.302042	-0.057931	4.816019
283.361850	7999.931216	10.307047	-0.057928	4.816015
283.365790	7999.893898	10.312051	-0.057929	4.816005
283.149652	7999.837622	10.317056	-0.057889	4.815989
283.414994	7999.884122	10.322061	-0.057938	4.816001
283.367563	7999.898228	10.327066	-0.057929	4.816006
283.272966	7999.952079	10.332071	-0.057912	4.816022
283.450373	7999.949968	10.337075	-0.057945	4.816020
283.304240	7999.960143	10.342080	-0.057918	4.816024
283.485528	7999.979473	10.347085	-0.057952	4.816029
283.346330	7999.939553	10.352090	-0.057926	4.816018
283.457299	7999.959742	10.357095	-0.057947	4.816023
283.537239	7999.975094	10.362099	-0.057962	4.816027
283.444723	7999.928543	10.367104	-0.057944	4.816014
283.481308	7999.973024	10.372109	-0.057951	4.816027
283.488590	7999.924013	10.377114	-0.057953	4.816013
283.425505	7999.919669	10.382119	-0.057941	4.816012
283.543704	7999.962428	10.387123	-0.057963	4.816024
283.554455	7999.917754	10.392128	-0.057965	4.816010
283.730425	7999.951947	10.397133	-0.057998	4.816020
283.497020	7999.963741	10.402138	-0.057955	4.816024
283.665516	7999.955057	10.407143	-0.057986	4.816021
283.616749	7999.916781	10.412147	-0.057977	4.816010
283.600072	7999.849169	10.417152	-0.057974	4.815990
283.540370	7999.963492	10.422157	-0.057963	4.816024
283.638550	7999.939639	10.427162	-0.057982	4.816016
283.654028	7999.951682	10.432167	-0.057985	4.816020
283.661011	7999.980667	10.437171	-0.057986	4.816028
283.550914	7999.897467	10.442176	-0.057965	4.816005
283.658503	7999.969952	10.447181	-0.057986	4.816025
283.719028	7999.948621	10.452186	-0.057997	4.816019
283.446795	7999.945819	10.457191	-0.057946	4.816019
283.448434	7999.967227	10.462195	-0.057947	4.816025
283.542491	7999.946505	10.467200	-0.057964	4.816019
283.555192	8000.025814	10.472205	-0.057967	4.816042
283.533782	8000.015816	10.477210	-0.057963	4.816039
283.582948	7999.968634	10.482215	-0.057972	4.816025
283.578012	8000.004882	10.487219	-0.057971	4.816036
283.536332	7999.954981	10.492224	-0.057964	4.816021
283.737279	8000.016341	10.497229	-0.058001	4.816038
283.611606	7999.959570	10.502234	-0.057978	4.816022
283.624797	7999.981188	10.507239	-0.057980	4.816029
283.577160	7999.964302	10.512243	-0.057972	4.816024
283.622595	7999.875381	10.517248	-0.057980	4.815998
283.647650	7999.958120	10.522253	-0.057985	4.816022
283.659382	7999.977574	10.527258	-0.057987	4.816027
283.737897	7999.951227	10.532263	-0.058002	4.816019
283.565878	7999.962000	10.537267	-0.057970	4.816023
283.542738	7999.899613	10.542272	-0.057966	4.816005
283.875125	7999.930238	10.547277	-0.058028	4.816012
283.826638	7999.938981	10.552282	-0.058019	4.816015
283.741588	7999.967362	10.557287	-0.058003	4.816024
283.767942	7999.978534	10.562291	-0.058008	4.816027
283.567091	7999.948178	10.567296	-0.057971	4.816019
283.559490	7999.989720	10.572301	-0.057969	4.816031
283.538858	7999.929516	10.577306	-0.057965	4.816014
283.649052	7999.924047	10.582311	-0.057986	4.816012
283.742847	7999.948199	10.587315	-0.058004	4.816018
283.765671	7999.964649	10.592320	-0.058008	4.816023
283.838654	8000.006588	10.597325	-0.058022	4.816035
283.779120	7999.975595	10.602330	-0.058011	4.816026
283.646370	7999.942203	10.607335	-0.057986	4.816017
283.707778	7999.975382	10.612339	-0.057997	4.816026
283.529243	7999.879185	10.617344	-0.057964	4.815999
283.607724	7999.884893	10.622349	-0.057979	4.816000
283.572942	7999.945174	10.627354	-0.057973	4.816018
283.946431	7999.916709	10.632359	-0.058042	4.816008
283.930582	8000.001911	10.637363	-0.058039	4.816033
283.692929	7999.969817	10.642368	-0.057995	4.816025
283.936015	8000.042629	10.647373	-0.058041	4.816045
283.968547	8000.010104	10.652378	-0.058047	4.816035
283.661960	8000.009882	10.657383	-0.057990	4.816037
283.570900	8000.003961	10.662387	-0.057973	4.816035
283.761266	7999.989264	10.667392	-0.058008	4.816030
283.752576	8000.005142	10.672397	-0.058007	4.816035
283.696118	7999.948560	10.677402	-0.057996	4.816019
283.725514	7999.943760	10.682407	-0.058002	4.816017
283.719706	8000.027007	10.687411	-0.058001	4.816041
283.727901	7999.941682	10.692416	-0.058002	4.816016
283.796075	7999.972847	10.697421	-0.058015	4.816025
283.795611	7999.973915	10.702426	-0.058015	4.816025
283.654081	8000.016229	10.707431	-0.057989	4.816039
283.790251	8000.014438	10.712435	-0.058014	4.816037
283.690744	7999.944252	10.717440	-0.057996	4.816017
283.697637	7999.976440	10.722445	-0.057997	4.816027
283.564037	7999.946239	10.727450	-0.057973	4.816019
283.607415	7999.921390	10.732455	-0.057981	4.816011
283.875402	7999.975421	10.737459	-0.058031	4.816025
283.742944	7999.978364	10.742464	-0.058006	4.816027
283.859841	7999.989045	10.747469	-0.058028	4.816030
283.877182	7999.962655	10.752474	-0.058031	4.816022
283.903566	8000.017637	10.757479	-0.058036	4.816038
284.012289	8000.035649	10.762483	-0.058057	4.816042
283.931853	7999.928411	10.767488	-0.058042	4.816011
284.046295	7999.989268	10.772493	-0.058063	4.816029
283.798395	7999.980496	10.777498	-0.058017	4.816027
283.971222	7999.954795	10.782503	-0.058049	4.816019
284.085809	8000.011380	10.787507	-0.058071	4.816035
283.885977	8000.019510	10.792512	-0.058034	4.816038
284.081374	8000.049783	10.797517	-0.058070	4.816046
283.996926	8000.010857	10.802522	-0.058054	4.816035
283.942654	7999.973548	10.807527	-0.058044	4.816025
283.935038	8000.004405	10.812531	-0.058043	4.816034
284.020464	7999.986732	10.817536	-0.058059	4.816028
284.083474	8000.026353	10.822541	-0.058071	4.816039
283.816189	8000.002269	10.827546	-0.058021	4.816034
283.859163	8000.032976	10.832551	-0.058029	4.816042
283.922955	8000.013842	10.837555	-0.058041	4.816036
284.007214	7999.933104	10.842560	-0.058057	4.816012
284.140802	8000.017818	10.847565	-0.058082	4.816036
284.061713	7999.982195	10.852570	-0.058067	4.816026
284.088755	7999.953844	10.857575	-0.058072	4.816018
284.012264	7999.999477	10.862579	-0.058058	4.816032
283.853822	7999.918602	10.867584	-0.058029	4.816009
284.076037	8000.003857	10.872589	-0.058070	4.816033
283.941869	7999.956548	10.877594	-0.058045	4.816020
283.874992	7999.882681	10.882599	-0.058033	4.815998
284.157492	7999.974374	10.887603	-0.058086	4.816024
283.838050	7999.889505	10.892608	-0.058026	4.816000
283.879264	7999.958647	10.897613	-0.058034	4.816020
284.037196	7999.951909	10.902618	-0.058063	4.816018
284.030257	7999.968887	10.907623	-0.058062	4.816023
284.019550	7999.992208	10.912627	-0.058060	4.816030
284.002364	7999.965191	10.917632	-0.058057	4.816022
283.926603	8000.004426	10.922637	-0.058043	4.816034
283.928249	7999.948900	10.927642	-0.058044	4.816017
283.918129	7999.931627	10.932647	-0.058042	4.816012
284.115644	8000.007886	10.937651	-0.058079	4.816034
284.174811	7999.940583	10.942656	-0.058090	4.816014
284.112354	8000.003567	10.947661	-0.058078	4.816032
284.024531	7999.970991	10.952666	-0.058062	4.816023
284.105474	7999.976745	10.957671	-0.058077	4.816025
283.826999	7999.983445	10.962675	-0.058025	4.816028
283.964423	7999.863070	10.967680	-0.058051	4.815992
283.888343	7999.933286	10.972685	-0.058037	4.816013
283.813596	7999.944758	10.977690	-0.058023	4.816017
283.920108	7999.876179	10.982695	-0.058043	4.815996
283.900131	7999.980539	10.987699	-0.058039	4.816027
283.725230	7999.946381	10.992704	-0.058007	4.816018
284.005478	7999.963237	10.997709	-0.058059	4.816021
284.242961	7999.967561	11.002714	-0.058103	4.816021
284.244652	7999.981491	11.007719	-0.058104	4.816025
284.226681	8000.021777	11.012723	-0.058101	4.816037
284.042959	7999.970361	11.017728	-0.058066	4.816023
284.284878	7999.972629	11.022733	-0.058112	4.816022
283.995105	7999.958821	11.027738	-0.058058	4.816020
284.040769	7999.969276	11.032743	-0.058066	4.816023
284.473653	7999.984633	11.037747	-0.058147	4.816025
284.045217	7999.931974	11.042752	-0.058067	4.816012
284.233376	7999.979212	11.047757	-0.058102	4.816025
284.036598	7999.990602	11.052762	-0.058066	4.816029
284.201752	7999.956214	11.057767	-0.058097	4.816018
284.315595	8000.001033	11.062771	-0.058118	4.816030
284.204251	7999.981920	11.067776	-0.058097	4.816025
284.369642	7999.969975	11.072781	-0.058128	4.816021
284.219908	7999.923451	11.077786	-0.058100	4.816008
284.043020	7999.925586	11.082791	-0.058067	4.816010
284.195372	7999.986064	11.087795	-0.058096	4.816027
284.123017	7999.965523	11.092800	-0.058083	4.816021
284.325969	7999.992728	11.097805	-0.058120	4.816028
284.408518	7999.973935	11.102810	-0.058136	4.816022
284.361109	7999.936750	11.107815	-0.058127	4.816011
284.383496	8000.003415	11.112819	-0.058131	4.816031
284.246685	7999.992387	11.117824	-0.058106	4.816028
284.334369	8000.033525	11.122829	-0.058122	4.816040
284.354285	8000.005044	11.127834	-0.058126	4.816031
284.214147	7999.956558	11.132839	-0.058100	4.816018
284.345710	8000.028412	11.137843	-0.058125	4.816038
284.238779	7999.931376	11.142848	-0.058105	4.816010
284.069237	7999.967838	11.147853	-0.058073	4.816022
284.216743	7999.968390	11.152858	-0.058101	4.816021
284.240607	7999.904720	11.157863	-0.058105	4.816003
284.441535	8000.001343	11.162867	-0.058143	4.816030
284.107183	7999.969628	11.167872	-0.058081	4.816022
284.273614	7999.982278	11.172877	-0.058112	4.816025
284.391734	7999.987639	11.177882	-0.058134	4.816026
284.237027	7999.992314	11.182887	-0.058105	4.816028
284.210048	8000.038847	11.187891	-0.058100	4.816042
284.154555	7999.983351	11.192896	-0.058090	4.816026
284.234103	8000.036095	11.197901	-0.058105	4.816041
284.254330	8000.001209	11.202906	-0.058109	4.816031
284.364902	7999.955142	11.207911	-0.058129	4.816017
284.262690	8000.014199	11.212915	-0.058111	4.816035
284.078257	7999.963839	11.217920	-0.058076	4.816021
284.141679	7999.945766	11.222925	-0.058088	4.816015
284.144923	7999.950107	11.227930	-0.058089	4.816016
284.161135	7999.977123	11.232935	-0.058092	4.816024
284.136891	8000.005540	11.237939	-0.058087	4.816033
284.095245	7999.946022	11.242944	-0.058080	4.816015
284.286102	8000.008269	11.247949	-0.058115	4.816033
284.348386	7999.993381	11.252954	-0.058127	4.816028
284.426100	7999.948854	11.257959	-0.058142	4.816015
284.414169	8000.014895	11.262963	-0.058140	4.816034
284.109007	7999.974093	11.267968	-0.058083	4.816024
284.326342	8000.001560	11.272973	-0.058123	4.816030
284.323860	7999.980152	11.277978	-0.058123	4.816024
284.081166	7999.973611	11.282983	-0.058078	4.816024
284.299717	8000.035293	11.287987	-0.058119	4.816040
284.235673	7999.952928	11.292992	-0.058107	4.816017
284.319221	8000.000401	11.297997	-0.058122	4.816030
284.211830	7999.989909	11.303002	-0.058102	4.816028
284.442068	7999.938538	11.308007	-0.058145	4.816011
284.615126	8000.026107	11.313011	-0.058178	4.816036
284.410466	7999.998886	11.318016	-0.058140	4.816029
284.522558	8000.020166	11.323021	-0.058161	4.816035
284.308115	7999.995973	11.328026	-0.058121	4.816029
284.392588	7999.996448	11.333031	-0.058137	4.816029
284.364661	8000.021593	11.338035	-0.058132	4.816036
284.444875	7999.973906	11.343040	-0.058147	4.816022
284.456966	7999.988025	11.348045	-0.058149	4.816026
284.265105	7999.971722	11.353050	-0.058113	4.816022
284.394067	7999.963389	11.358055	-0.058137	4.816019
284.332040	8000.015697	11.363059	-0.058126	4.816035
284.383161	7999.979235	11.368064	-0.058135	4.816024
284.426407	8000.044142	11.373069	-0.058144	4.816042
284.398975	8000.018006	11.378074	-0.058139	4.816035
284.294386	8000.007564	11.383079	-0.058119	4.816032
284.440893	7999.986727	11.388083	-0.058147	4.816025
284.122831	7999.986296	11.393088	-0.058087	4.816027
284.255326	8000.009015	11.398093	-0.058112	4.816033
284.363050	7999.990679	11.403098	-0.058132	4.816027
284.341815	7999.960381	11.408103	-0.058128	4.816018
284.436807	7999.964253	11.413107	-0.058146	4.816019
284.319854	7999.976026	11.418112	-0.058124	4.816023
284.402579	7999.981812	11.423117	-0.058140	4.816024
284.389847	7999.999754	11.428122	-0.058138	4.816030
284.611702	8000.000590	11.433127	-0.058179	4.816029
284.469809	7999.981990	11.438131	-0.058153	4.816024
284.436789	7999.942930	11.443136	-0.058147	4.816013
284.592611	8000.007746	11.448141	-0.058176	4.816031
284.406397	7999.987272	11.453146	-0.058141	4.816026
284.445107	7999.955927	11.458151	-0.058148	4.816016
284.238359	7999.986370	11.463155	-0.058110	4.816026
284.235713	7999.952136	11.468160	-0.058110	4.816016
284.373769	7999.957859	11.473165	-0.058135	4.816017
284.539791	7999.974777	11.478170	-0.058166	4.816021
284.370070	7999.957808	11.483175	-0.058135	4.816017
284.276057	7999.979615	11.488179	-0.058117	4.816024
284.455590	7999.968995	11.493184	-0.058151	4.816020
284.429659	8000.000588	11.498189	-0.058146	4.816030
284.525856	7999.967083	11.503194	-0.058164	4.816019
284.581194	7999.998016	11.508199	-0.058175	4.816028
284.789255	8000.047755	11.513203	-0.058213	4.816041
284.438545	7999.981548	11.518208	-0.058148	4.816024
284.410791	7999.979982	11.523213	-0.058143	4.816024
284.500173	7999.954902	11.528218	-0.058160	4.816016
284.412889	7999.970419	11.533223	-0.058144	4.816021
284.346986	7999.992737	11.538227	-0.058131	4.816028
284.520598	8000.004450	11.543232	-0.058164	4.816030
284.500782	8000.032948	11.548237	-0.058160	4.816039
284.266639	7999.993437	11.553242	-0.058117	4.816028
284.379602	7999.997636	11.558247	-0.058138	4.816029
284.527089	7999.996051	11.563251	-0.058165	4.816028
284.483946	7999.974972	11.568256	-0.058157	4.816022
284.221500	7999.953112	11.573261	-0.058109	4.816017
284.409337	7999.995002	11.578266	-0.058144	4.816028
284.472613	8000.033560	11.583271	-0.058156	4.816039
284.489981	8000.044569	11.588275	-0.058159	4.816042
284.547179	8000.000738	11.593280	-0.058170	4.816029
284.426300	8000.033810	11.598285	-0.058147	4.816039
284.267214	7999.964676	11.603290	-0.058118	4.816020
284.377550	7999.926085	11.608295	-0.058138	4.816008
284.585589	7999.959795	11.613299	-0.058177	4.816017
284.601741	7999.959028	11.618304	-0.058180	4.816016
284.424355	8000.035951	11.623309	-0.058147	4.816040
284.410972	8000.022893	11.628314	-0.058145	4.816036
284.467118	7999.987591	11.633319	-0.058155	4.816025
284.522359	8000.031346	11.638323	-0.058166	4.816038
284.580437	7999.990736	11.643328	-0.058177	4.816026
284.671470	7999.995605	11.648333	-0.058194	4.816027
284.735243	8000.019212	11.653338	-0.058206	4.816033
284.534834	8000.004890	11.658343	-0.058168	4.816030
284.630467	8000.020528	11.663347	-0.058186	4.816034
284.603850	8000.023258	11.668352	-0.058181	4.816035
284.663709	8000.035040	11.673357	-0.058193	4.816038
284.514059	8000.032326	11.678362	-0.058165	4.816038
284.624238	8000.076011	11.683367	-0.058185	4.816050
284.453682	8000.065438	11.688371	-0.058154	4.816048
284.331496	8000.030099	11.693376	-0.058131	4.816039
284.521541	8000.039974	11.698381	-0.058167	4.816040
284.405026	7999.994053	11.703386	-0.058145	4.816028
284.356127	8000.008131	11.708391	-0.058136	4.816032
284.577185	8000.049558	11.713395	-0.058177	4.816043
284.397000	8000.013165	11.718400	-0.058144	4.816033
284.468094	8000.041179	11.723405	-0.058157	4.816041
284.502415	8000.006549	11.728410	-0.058163	4.816031
284.587045	8000.029466	11.733415	-0.058179	4.816037
284.558007	8000.042837	11.738419	-0.058174	4.816041
284.494581	7999.986127	11.743424	-0.058162	4.816025
284.876819	8000.002702	11.748429	-0.058234	4.816028
284.730091	7999.995768	11.753434	-0.058206	4.816026
284.553802	7999.984022	11.758439	-0.058174	4.816024
284.592446	8000.024269	11.763443	-0.058181	4.816035
284.640913	7999.982416	11.768448	-0.058190	4.816023
284.803137	7999.999265	11.773453	-0.058220	4.816027
284.632578	7999.982281	11.778458	-0.058189	4.816023
284.654133	7999.919636	11.783463	-0.058193	4.816005
284.785094	8000.013920	11.788467	-0.058217	4.816031
284.433440	7999.940216	11.793472	-0.058152	4.816012
284.677566	7999.970308	11.798477	-0.058197	4.816019
284.633073	7999.975918	11.803482	-0.058189	4.816021
284.609432	7999.929548	11.808487	-0.058185	4.816008
284.615932	7999.991650	11.813491	-0.058186	4.816026
284.458939	7999.998421	11.818496	-0.058157	4.816029
284.449754	8000.013221	11.823501	-0.058155	4.816033
284.665682	8000.016086	11.828506	-0.058196	4.816033
284.588053	7999.967667	11.833511	-0.058181	4.816019
284.643447	7999.990053	11.838515	-0.058192	4.816025
284.613174	7999.937151	11.843520	-0.058186	4.816010
284.955157	7999.965817	11.848525	-0.058250	4.816016
284.768108	7999.996617	11.853530	-0.058215	4.816026
284.824861	7999.982698	11.858535	-0.058226	4.816022
284.639770	8000.015671	11.863539	-0.058191	4.816033
284.571508	7999.970627	11.868544	-0.058179	4.816020
284.646049	7999.994430	11.873549	-0.058193	4.816026
284.697637	8000.011404	11.878554	-0.058202	4.816031
284.636639	7999.986794	11.883559	-0.058191	4.816024
284.632159	8000.042286	11.888563	-0.058190	4.816040
284.560432	7999.991836	11.893568	-0.058177	4.816026
284.583223	8000.010424	11.898573	-0.058181	4.816031
284.619508	7999.998269	11.903578	-0.058188	4.816028
284.687855	7999.980285	11.908583	-0.058201	4.816022
284.732539	8000.008888	11.913587	-0.058209	4.816030
284.470721	7999.994519	11.918592	-0.058161	4.816027
284.650987	7999.998873	11.923597	-0.058194	4.816028
284.610214	7999.997071	11.928602	-0.058187	4.816027
284.667202	7999.983155	11.933607	-0.058197	4.816023
284.611100	8000.012062	11.938611	-0.058187	4.816032
284.491579	8000.008828	11.943616	-0.058165	4.816031
284.695516	7999.986899	11.948621	-0.058203	4.816024
284.680984	7999.995191	11.953626	-0.058200	4.816026
284.490095	7999.992797	11.958631	-0.058165	4.816027
284.605364	8000.034437	11.963635	-0.058186	4.816038
284.670601	7999.999300	11.968640	-0.058199	4.816028
284.938091	8000.038366	11.973645	-0.058249	4.816038
284.870185	8000.018974	11.978650	-0.058236	4.816032
284.795400	8000.033650	11.983655	-0.058222	4.816037
284.815178	8000.067143	11.988659	-0.058226	4.816047
284.868623	8000.010421	11.993664	-0.058236	4.816030
284.958750	8000.071907	11.998669	-0.058253	4.816047
284.898894	7999.998164	12.003674	-0.058242	4.816026
284.998066	7999.945479	12.008679	-0.058260	4.816010
284.990533	8000.050069	12.013683	-0.058259	4.816041
284.996838	7999.973255	12.018688	-0.058260	4.816018
285.146188	8000.015516	12.023693	-0.058288	4.816030
284.913719	8000.007022	12.028698	-0.058245	4.816029
284.906791	8000.020795	12.033703	-0.058244	4.816033
285.091990	8000.030582	12.038707	-0.058278	4.816035
284.918556	8000.003928	12.043712	-0.058246	4.816028
284.653011	8000.014067	12.048717	-0.058197	4.816032
284.932541	8000.011678	12.053722	-0.058249	4.816030
284.929954	7999.960348	12.058727	-0.058248	4.816015
284.959859	8000.034630	12.063731	-0.058254	4.816036
284.997424	7999.978687	12.068736	-0.058261	4.816020
284.791896	7999.997398	12.073741	-0.058223	4.816026
284.910690	7999.989949	12.078746	-0.058245	4.816024
284.992513	7999.976485	12.083751	-0.058260	4.816019
285.022923	8000.026199	12.088755	-0.058266	4.816034
284.971143	8000.002826	12.093760	-0.058257	4.816027
284.993612	8000.045985	12.098765	-0.058261	4.816040
284.986396	8000.022353	12.103770	-0.058260	4.816033
284.748661	7999.976364	12.108775	-0.058215	4.816020
284.943762	8000.023731	12.113779	-0.058252	4.816033
284.872772	7999.927346	12.118784	-0.058239	4.816005
284.943529	7999.931846	12.123789	-0.058252	4.816006
284.851013	7999.937652	12.128794	-0.058235	4.816009
284.982872	7999.962497	12.133799	-0.058259	4.816015
284.866053	8000.010603	12.138803	-0.058238	4.816030
284.738381	7999.993330	12.143808	-0.058214	4.816025
284.876841	8000.010815	12.148813	-0.058240	4.816030
285.145450	7999.954800	12.153818	-0.058290	4.816012
284.980208	7999.945391	12.158823	-0.058259	4.816010
285.037642	8000.028723	12.163827	-0.058270	4.816034
284.847802	7999.988947	12.168832	-0.058235	4.816024
284.962393	7999.992108	12.173837	-0.058256	4.816024
284.853647	7999.986932	12.178842	-0.058236	4.816023
284.815582	7999.937095	12.183847	-0.058229	4.816009
285.172369	8000.002361	12.188851	-0.058296	4.816026
284.997888	7999.998127	12.193856	-0.058263	4.816025
284.960681	7999.995322	12.198861	-0.058256	4.816025
284.895327	7999.995210	12.203866	-0.058244	4.816025
284.780742	7999.958940	12.208871	-0.058223	4.816015
284.867674	8000.012888	12.213875	-0.058239	4.816030
284.990150	7999.978792	12.218880	-0.058262	4.816020
284.820440	7999.921218	12.223885	-0.058231	4.816004
284.898842	7999.986765	12.228890	-0.058245	4.816023
284.976204	7999.967877	12.233895	-0.058260	4.816017
285.075280	8000.010292	12.238899	-0.058278	4.816029
284.930082	8000.000179	12.243904	-0.058251	4.816026
284.877610	7999.957559	12.248909	-0.058242	4.816014
284.763841	7999.995035	12.253914	-0.058221	4.816026
284.907664	7999.924996	12.258919	-0.058247	4.816005
284.962007	7999.933472	12.263923	-0.058258	4.816007
284.880254	7999.910623	12.268928	-0.058243	4.816000
285.154884	7999.945544	12.273933	-0.058294	4.816009
285.254566	7999.956982	12.278938	-0.058312	4.816012
285.016408	7999.912053	12.283943	-0.058268	4.816000
285.186678	7999.972860	12.288947	-0.058300	4.816017
284.979402	7999.966961	12.293952	-0.058261	4.816016
284.970708	8000.028787	12.298957	-0.058260	4.816035
285.076419	8000.001867	12.303962	-0.058280	4.816026
285.005889	7999.961055	12.308967	-0.058267	4.816015
285.081481	8000.006249	12.313971	-0.058281	4.816027
284.871608	7999.949012	12.318976	-0.058242	4.816012
284.995881	7999.940594	12.323981	-0.058265	4.816009
285.063018	7999.968537	12.328986	-0.058278	4.816016
285.044811	7999.971420	12.333991	-0.058274	4.816017
285.334804	7999.980975	12.338995	-0.058328	4.816019
285.107454	7999.946929	12.344000	-0.058286	4.816010
285.067713	7999.986820	12.349005	-0.058279	4.816022
285.210028	7999.935987	12.354010	-0.058305	4.816006
285.180096	7999.883092	12.359015	-0.058300	4.815991
285.190548	8000.021134	12.364019	-0.058302	4.816031
284.918821	7999.948881	12.369024	-0.058251	4.816011
285.193968	7999.970990	12.374029	-0.058303	4.816016
285.187560	7999.948441	12.379034	-0.058302	4.816010
285.056763	7999.880889	12.384039	-0.058277	4.815991
284.998606	7999.995243	12.389043	-0.058267	4.816025
285.179670	7999.951527	12.394048	-0.058300	4.816011
285.121400	7999.940858	12.399053	-0.058290	4.816008
285.182210	7999.965480	12.404058	-0.058301	4.816015
285.185076	7999.928141	12.409063	-0.058302	4.816004
285.157135	7999.994960	12.414067	-0.058296	4.816024
285.038509	7999.960754	12.419072	-0.058274	4.816014
285.138497	7999.944414	12.424077	-0.058293	4.816009
285.243066	7999.959147	12.429082	-0.058313	4.816013
285.063442	7999.912077	12.434087	-0.058279	4.816000
285.192756	7999.900545	12.439091	-0.058303	4.815996
285.152854	7999.926542	12.444096	-0.058296	4.816004
285.201999	7999.930649	12.449101	-0.058305	4.816005
285.011032	7999.980612	12.454106	-0.058270	4.816020
285.050323	8000.015528	12.459111	-0.058277	4.816030
285.135035	8000.052340	12.464115	-0.058293	4.816040
284.893239	7999.946437	12.469120	-0.058248	4.816011
285.070235	7999.934704	12.474125	-0.058281	4.816006
285.070957	7999.978536	12.479130	-0.058281	4.816019
285.053532	7999.937621	12.484135	-0.058278	4.816007
285.277183	7999.994056	12.489139	-0.058320	4.816023
285.145103	7999.948919	12.494144	-0.058296	4.816010
285.079001	8000.042827	12.499149	-0.058283	4.816038
285.194648	8000.013950	12.504154	-0.058305	4.816029
285.156157	7999.996161	12.509159	-0.058298	4.816024
285.249828	7999.995735	12.514163	-0.058315	4.816023
285.211109	7999.968325	12.519168	-0.058308	4.816015
285.062143	7999.957075	12.524173	-0.058281	4.816013
284.969122	7999.942569	12.529178	-0.058263	4.816009
284.986456	7999.925795	12.534183	-0.058267	4.816004
285.061981	7999.982741	12.539187	-0.058281	4.816020
284.972694	7999.993948	12.544192	-0.058264	4.816024
285.098648	8000.044332	12.549197	-0.058288	4.816038
285.009028	8000.023476	12.554202	-0.058271	4.816033
284.896191	7999.981895	12.559207	-0.058250	4.816021
285.023492	8000.006658	12.564211	-0.058274	4.816028
285.023809	7999.919050	12.569216	-0.058274	4.816002
285.078799	7999.914715	12.574221	-0.058284	4.816000
285.265779	7999.954454	12.579226	-0.058319	4.816011
285.223782	7999.950492	12.584231	-0.058312	4.816010
285.034159	7999.998343	12.589235	-0.058276	4.816025
285.007920	7999.975434	12.594240	-0.058272	4.816019
285.218968	7999.950429	12.599245	-0.058311	4.816010
285.244531	8000.007535	12.604250	-0.058316	4.816027
285.070903	8000.006523	12.609255	-0.058284	4.816027
285.172684	8000.024410	12.614259	-0.058303	4.816032
285.150110	7999.995156	12.619264	-0.058298	4.816024
285.130870	8000.016185	12.624269	-0.058295	4.816030
285.269506	8000.020852	12.629274	-0.058321	4.816030
285.118620	7999.996744	12.634279	-0.058293	4.816024
285.139255	8000.039870	12.639283	-0.058297	4.816037
285.265983	7999.996234	12.644288	-0.058320	4.816023
285.231998	8000.008447	12.649293	-0.058314	4.816027
285.174379	8000.006339	12.654298	-0.058304	4.816027
285.087496	8000.004766	12.659303	-0.058287	4.816027
285.295890	8000.034210	12.664307	-0.058326	4.816034
285.078393	7999.984314	12.669312	-0.058286	4.816021
285.126636	7999.984131	12.674317	-0.058295	4.816020
285.318219	7999.988691	12.679322	-0.058331	4.816021
285.206801	7999.998427	12.684327	-0.058310	4.816024
285.266783	8000.042269	12.689331	-0.058321	4.816037
285.019931	8000.033513	12.694336	-0.058275	4.816035
285.077885	8000.043123	12.699341	-0.058286	4.816038
285.202289	8000.027228	12.704346	-0.058310	4.816033
285.012726	8000.057982	12.709351	-0.058274	4.816043
284.985178	8000.057489	12.714355	-0.058269	4.816043
285.109600	7999.991372	12.719360	-0.058293	4.816023
285.187591	7999.979975	12.724365	-0.058307	4.816019
285.115939	8000.005394	12.729370	-0.058294	4.816027
285.230747	7999.924142	12.734375	-0.058315	4.816002
285.319894	7999.988817	12.739379	-0.058332	4.816021
285.169240	8000.003182	12.744384	-0.058304	4.816026
285.247949	7999.928753	12.749389	-0.058319	4.816004
285.158555	7999.948506	12.754394	-0.058302	4.816010
285.131156	7999.995033	12.759399	-0.058297	4.816024
285.337585	8000.024441	12.764403	-0.058336	4.816031
285.159698	7999.952825	12.769408	-0.058303	4.816011
285.199955	8000.026228	12.774413	-0.058310	4.816032
285.410235	8000.010826	12.779418	-0.058350	4.816027
285.167354	7999.930548	12.784423	-0.058304	4.816005
285.215510	8000.037220	12.789427	-0.058313	4.816035
285.036594	7999.952763	12.794432	-0.058280	4.816012
285.032477	7999.956970	12.799437	-0.058279	4.816013
284.982519	7999.981715	12.804442	-0.058270	4.816020
284.842052	7999.959935	12.809447	-0.058244	4.816015
285.204595	7999.982564	12.814451	-0.058312	4.816020
285.096159	7999.985943	12.819456	-0.058292	4.816021
285.176485	8000.025880	12.824461	-0.058307	4.816032
285.148095	8000.018960	12.829466	-0.058302	4.816030
285.195791	7999.987778	12.834471	-0.058310	4.816021
285.387071	8000.019048	12.839475	-0.058346	4.816029
285.290824	7999.975631	12.844480	-0.058328	4.816017
285.226709	8000.018284	12.849485	-0.058316	4.816030
285.303910	8000.000462	12.854490	-0.058331	4.816024
285.198427	7999.998551	12.859495	-0.058311	4.816024
285.419590	8000.047462	12.864499	-0.058353	4.816037
285.218216	8000.009613	12.869504	-0.058315	4.816027
285.092988	8000.027646	12.874509	-0.058292	4.816033
285.240550	8000.034612	12.879514	-0.058320	4.816035
285.244954	8000.006917	12.884519	-0.058320	4.816026
285.200423	8000.068092	12.889523	-0.058312	4.816045
285.114797	8000.036623	12.894528	-0.058296	4.816036
285.106020	8000.047157	12.899533	-0.058295	4.816039
285.231970	8000.031290	12.904538	-0.058318	4.816034
285.194545	7999.978257	12.909543	-0.058311	4.816018
285.223765	8000.053596	12.914547	-0.058317	4.816040
285.328911	8000.015979	12.919552	-0.058337	4.816029
285.296864	8000.058147	12.924557	-0.058331	4.816041
285.199562	8000.069208	12.929562	-0.058313	4.816045
284.999340	8000.001461	12.934567	-0.058276	4.816026
285.131207	8000.061569	12.939571	-0.058300	4.816043
285.090403	8000.053355	12.944576	-0.058293	4.816041
285.408658	7999.997174	12.949581	-0.058352	4.816023
285.471908	8000.020773	12.954586	-0.058364	4.816029
285.231515	7999.985420	12.959591	-0.058319	4.816020
285.342428	8000.021639	12.964595	-0.058340	4.816030
285.473104	7999.995173	12.969600	-0.058364	4.816022
285.441390	8000.046964	12.974605	-0.058359	4.816037
285.428901	8000.025373	12.979610	-0.058356	4.816031
285.604426	7999.992242	12.984615	-0.058389	4.816020
285.690474	8000.044038	12.989619	-0.058405	4.816035
285.353622	8000.022959	12.994624	-0.058342	4.816030
285.541710	8000.053102	12.999629	-0.058378	4.816038
285.635422	8000.040923	13.004634	-0.058395	4.816034
285.619008	7999.995752	13.009639	-0.058392	4.816021
285.567950	8000.042918	13.014643	-0.058383	4.816035
285.346838	8000.022875	13.019648	-0.058342	4.816030
285.494389	7999.965727	13.024653	-0.058369	4.816013
285.412157	8000.049725	13.029658	-0.058354	4.816038
285.259404	8000.005280	13.034663	-0.058326	4.816026
285.316707	8000.066170	13.039667	-0.058336	4.816043
285.240762	8000.015642	13.044672	-0.058322	4.816029
285.310942	8000.012652	13.049677	-0.058335	4.816028
285.273193	8000.037619	13.054682	-0.058328	4.816035
285.246543	8000.012565	13.059687	-0.058324	4.816028
285.254120	8000.028740	13.064691	-0.058325	4.816033
285.448945	8000.013057	13.069696	-0.058361	4.816027
285.466271	8000.043300	13.074701	-0.058365	4.816036
285.190244	8000.039356	13.079706	-0.058313	4.816036
285.314288	7999.983917	13.084711	-0.058337	4.816019
285.476554	8000.071294	13.089715	-0.058367	4.816044
285.443486	8000.016203	13.094720	-0.058361	4.816028
285.514852	8000.018577	13.099725	-0.058374	4.816028
285.475029	8000.044575	13.104730	-0.058367	4.816036
285.355220	8000.018895	13.109735	-0.058345	4.816029
285.297991	8000.025342	13.114739	-0.058334	4.816031
285.248356	8000.018036	13.119744	-0.058325	4.816030
285.350316	8000.029516	13.124749	-0.058344	4.816032
285.295355	8000.024250	13.129754	-0.058334	4.816031
285.335155	8000.011090	13.134759	-0.058341	4.816027
285.458249	8000.084931	13.139763	-0.058364	4.816048
285.283049	8000.039009	13.144768	-0.058332	4.816035
285.150400	8000.096445	13.149773	-0.058307	4.816053
285.377670	8000.047158	13.154778	-0.058350	4.816037
285.377786	8000.069608	13.159783	-0.058350	4.816044
285.543745	8000.067292	13.164787	-0.058381	4.816042
285.435459	8000.027930	13.169792	-0.058361	4.816031
285.234260	8000.037101	13.174797	-0.058323	4.816035
285.317064	8000.065329	13.179802	-0.058339	4.816043
285.463877	8000.061596	13.184807	-0.058366	4.816041
285.435644	8000.077119	13.189811	-0.058361	4.816046
285.468105	8000.049935	13.194816	-0.058367	4.816038
285.300303	8000.015902	13.199821	-0.058336	4.816029
285.450084	8000.047485	13.204826	-0.058364	4.816037
285.371078	8000.040713	13.209831	-0.058349	4.816035
285.494700	8000.046176	13.214835	-0.058372	4.816036
285.484269	7999.997908	13.219840	-0.058370	4.816022
285.510653	8000.060373	13.224845	-0.058375	4.816040
285.601910	8000.053493	13.229850	-0.058393	4.816038
285.460676	7999.973994	13.234855	-0.058366	4.816015
285.650497	8000.040501	13.239859	-0.058402	4.816034
285.536878	8000.012796	13.244864	-0.058381	4.816026
285.386291	8000.037848	13.249869	-0.058353	4.816035
285.445181	8000.079533	13.254874	-0.058364	4.816046
285.463615	8000.040339	13.259879	-0.058367	4.816035
285.593056	8000.074758	13.264883	-0.058391	4.816044
285.412868	8000.031951	13.269888	-0.058358	4.816033
285.497561	8000.059146	13.274893	-0.058374	4.816040
285.522747	8000.074572	13.279898	-0.058379	4.816045
285.523951	8000.025447	13.284903	-0.058379	4.816030
285.498802	8000.065603	13.289907	-0.058374	4.816042
285.383061	8000.052820	13.294912	-0.058353	4.816039
285.401918	8000.042485	13.299917	-0.058356	4.816036
285.455527	8000.035988	13.304922	-0.058366	4.816034
285.627025	8000.038047	13.309927	-0.058398	4.816033
285.779471	8000.071817	13.314931	-0.058427	4.816042
285.497661	8000.013270	13.319936	-0.058375	4.816027
285.695861	8000.080998	13.324941	-0.058412	4.816045
285.498417	8000.065660	13.329946	-0.058375	4.816042
285.350787	8000.054433	13.334951	-0.058347	4.816040
285.465681	8000.083246	13.339955	-0.058369	4.816047
285.260935	8000.058158	13.344960	-0.058331	4.816041
285.378913	8000.104123	13.349965	-0.058353	4.816054
285.432477	8000.095488	13.354970	-0.058363	4.816051
285.387759	8000.030568	13.359975	-0.058355	4.816032
285.492085	8000.062394	13.364979	-0.058374	4.816041
285.673953	8000.043270	13.369984	-0.058408	4.816035
285.612588	8000.026133	13.374989	-0.058397	4.816030
285.612262	8000.062467	13.379994	-0.058397	4.816040
285.426397	8000.032379	13.384999	-0.058362	4.816033
285.622916	8000.056265	13.390003	-0.058399	4.816039
285.600334	8000.036627	13.395008	-0.058395	4.816033
285.265709	8000.075429	13.400013	-0.058333	4.816046
285.561431	8000.079747	13.405018	-0.058388	4.816046
285.706362	8000.067432	13.410023	-0.058415	4.816041
285.547183	8000.069887	13.415027	-0.058385	4.816043
285.541210	8000.072992	13.420032	-0.058384	4.816044
285.734466	8000.056212	13.425037	-0.058420	4.816038
285.553517	8000.088192	13.430042	-0.058387	4.816048
285.461799	8000.068365	13.435047	-0.058370	4.816043
285.563726	8000.081982	13.440051	-0.058389	4.816046
285.347348	8000.026762	13.445056	-0.058349	4.816031
285.500553	8000.038105	13.450061	-0.058377	4.816034
285.589341	8000.033317	13.455066	-0.058394	4.816032
285.401712	8000.050214	13.460071	-0.058359	4.816038
285.616431	8000.046648	13.465075	-0.058399	4.816036
285.518500	8000.027777	13.470080	-0.058381	4.816031
285.623851	8000.006193	13.475085	-0.058401	4.816024
285.593822	8000.055878	13.480090	-0.058395	4.816039
285.715265	8000.032449	13.485095	-0.058418	4.816031
285.757527	8000.071695	13.490099	-0.058426	4.816042
285.661007	8000.053918	13.495104	-0.058408	4.816038
285.595212	8000.060209	13.500109	-0.058396	4.816040
285.388482	8000.062868	13.505114	-0.058357	4.816042
285.630034	7999.997812	13.510119	-0.058402	4.816021
285.680249	8000.070328	13.515123	-0.058412	4.816042
285.552158	8000.023126	13.520128	-0.058388	4.816029
285.767134	8000.028113	13.525133	-0.058428	4.816030
285.808259	8000.040623	13.530138	-0.058436	4.816033
285.661909	8000.052929	13.535143	-0.058409	4.816037
285.569199	8000.069416	13.540147	-0.058391	4.816043
285.626737	8000.040551	13.545152	-0.058402	4.816034
285.583546	8000.025881	13.550157	-0.058394	4.816030
285.641156	8000.029074	13.555162	-0.058405	4.816030
285.572310	8000.016076	13.560167	-0.058392	4.816027
285.602421	8000.076472	13.565171	-0.058398	4.816045
285.437673	8000.038220	13.570176	-0.058367	4.816034
285.657938	8000.066812	13.575181	-0.058409	4.816041
285.613108	8000.033947	13.580186	-0.058400	4.816032
285.463640	8000.016276	13.585191	-0.058372	4.816028
285.597374	8000.051842	13.590195	-0.058398	4.816037
285.595379	8000.041128	13.595200	-0.058397	4.816034
285.530646	8000.043164	13.600205	-0.058385	4.816035
285.488376	8000.072323	13.605210	-0.058377	4.816044
285.569817	8000.033207	13.610215	-0.058393	4.816032
285.651434	8000.063551	13.615219	-0.058408	4.816040
285.441198	8000.020197	13.620224	-0.058369	4.816029
285.393448	8000.020405	13.625229	-0.058360	4.816029
285.612553	8000.021193	13.630234	-0.058401	4.816028
285.602033	8000.028489	13.635239	-0.058399	4.816030
285.575779	8000.047254	13.640243	-0.058394	4.816036
285.503577	8000.042743	13.645248	-0.058381	4.816035
285.653672	8000.051893	13.650253	-0.058409	4.816037
285.554940	8000.052242	13.655258	-0.058391	4.816038
285.583543	8000.004684	13.660263	-0.058396	4.816024
285.695645	8000.090080	13.665267	-0.058417	4.816048
285.461813	8000.036680	13.670272	-0.058374	4.816034
285.538992	8000.040229	13.675277	-0.058388	4.816034
285.883358	8000.076422	13.680282	-0.058452	4.816043
285.792103	8000.021340	13.685287	-0.058435	4.816027
285.717476	8000.073420	13.690291	-0.058421	4.816043
285.740248	8000.037510	13.695296	-0.058426	4.816032
285.646957	8000.077495	13.700301	-0.058409	4.816045
285.678449	8000.087694	13.705306	-0.058414	4.816047
285.471222	8000.052943	13.710311	-0.058376	4.816038
285.690053	8000.071892	13.715315	-0.058417	4.816043
285.609749	8000.017010	13.720320	-0.058402	4.816027
285.460918	8000.064533	13.725325	-0.058374	4.816042
285.923756	8000.062276	13.730330	-0.058461	4.816039
285.613508	8000.007484	13.735335	-0.058403	4.816024
285.533485	8000.074426	13.740339	-0.058388	4.816044
285.498351	8000.063109	13.745344	-0.058382	4.816041
285.707912	8000.080821	13.750349	-0.058421	4.816045
285.832664	8000.055315	13.755354	-0.058444	4.816037
285.741675	8000.021610	13.760359	-0.058427	4.816028
285.932667	8000.075316	13.765363	-0.058463	4.816042
285.933074	8000.051822	13.770368	-0.058463	4.816035
285.816532	8000.043299	13.775373	-0.058441	4.816034
285.730918	8000.038543	13.780378	-0.058425	4.816033
285.719581	8000.046894	13.785383	-0.058423	4.816035
285.841336	8000.099340	13.790387	-0.058446	4.816050
285.581416	8000.081796	13.795392	-0.058398	4.816046
285.837869	8000.055481	13.800397	-0.058446	4.816037
285.535582	8000.091664	13.805402	-0.058390	4.816049
285.799494	8000.045181	13.810407	-0.058439	4.816034
285.941996	8000.068085	13.815411	-0.058465	4.816040
285.755355	8000.049737	13.820416	-0.058431	4.816036
285.725180	8000.081253	13.825421	-0.058425	4.816045
285.748311	8000.069928	13.830426	-0.058430	4.816042
285.710243	8000.028637	13.835431	-0.058422	4.816030
285.619565	8000.078287	13.840435	-0.058406	4.816045
285.523116	8000.077609	13.845440	-0.058388	4.816045
285.657935	8000.095030	13.850445	-0.058413	4.816049
285.822831	8000.067049	13.855450	-0.058444	4.816040
285.718511	8000.024552	13.860455	-0.058424	4.816029
285.956212	8000.071628	13.865459	-0.058469	4.816041
285.915188	8000.059135	13.870464	-0.058461	4.816038
285.694746	8000.064750	13.875469	-0.058420	4.816040
285.882677	8000.050011	13.880474	-0.058455	4.816035
285.680520	8000.011078	13.885479	-0.058418	4.816025
285.735469	8000.078338	13.890483	-0.058428	4.816044
285.650958	8000.035133	13.895488	-0.058412	4.816032
285.657922	8000.032062	13.900493	-0.058414	4.816031
285.652450	8000.049068	13.905498	-0.058413	4.816036
285.668864	8000.040826	13.910503	-0.058416	4.816034
285.913151	8000.077335	13.915507	-0.058462	4.816043
285.742259	8000.058205	13.920512	-0.058430	4.816038
285.709801	8000.090749	13.925517	-0.058424	4.816048
285.872833	8000.093723	13.930522	-0.058454	4.816048
285.761635	8000.010495	13.935527	-0.058434	4.816024
285.882214	8000.084292	13.940531	-0.058456	4.816045
285.806550	8000.065826	13.945536	-0.058442	4.816040
285.852338	8000.078422	13.950541	-0.058451	4.816044
285.946350	8000.078003	13.955546	-0.058468	4.816043
285.749788	8000.057337	13.960551	-0.058432	4.816038
285.805415	8000.103238	13.965555	-0.058442	4.816051
285.703112	8000.075738	13.970560	-0.058423	4.816044
285.605458	8000.082518	13.975565	-0.058405	4.816046
285.743218	8000.090375	13.980570	-0.058431	4.816048
285.650766	8000.063055	13.985575	-0.058414	4.816040
285.797864	8000.090317	13.990579	-0.058441	4.816047
285.814914	8000.057509	13.995584	-0.058445	4.816038
285.855589	8000.033679	14.000589	-0.058452	4.816030
285.925272	8000.068081	14.005594	-0.058465	4.816040
285.639181	8000.072501	14.010599	-0.058412	4.816043
285.879700	8000.085434	14.015603	-0.058457	4.816045
285.830494	8000.067449	14.020608	-0.058448	4.816040
285.703227	8000.039495	14.025613	-0.058424	4.816033
285.668856	8000.094444	14.030618	-0.058418	4.816049
285.959605	8000.067685	14.035623	-0.058472	4.816040
285.937910	8000.086532	14.040627	-0.058468	4.816045
285.720140	8000.039835	14.045632	-0.058428	4.816033
285.886972	8000.057838	14.050637	-0.058459	4.816037
285.916091	8000.072267	14.055642	-0.058464	4.816041
285.646590	8000.052412	14.060647	-0.058414	4.816037
285.825337	8000.071701	14.065651	-0.058448	4.816042
285.702960	8000.038493	14.070656	-0.058425	4.816033
285.764488	8000.037483	14.075661	-0.058436	4.816032
285.842449	8000.064556	14.080666	-0.058451	4.816040
285.870034	8000.030870	14.085671	-0.058456	4.816030
285.909710	8000.045492	14.090675	-0.058464	4.816034
285.765830	8000.025785	14.095680	-0.058437	4.816029
285.961953	8000.035772	14.100685	-0.058474	4.816030
285.919589	8000.031804	14.105690	-0.058466	4.816030
285.900966	8000.026130	14.110695	-0.058462	4.816028
285.878451	8000.039620	14.115699	-0.058458	4.816032
286.132338	8000.035698	14.120704	-0.058506	4.816030
285.927685	8000.013817	14.125709	-0.058468	4.816024
285.850079	8000.056225	14.130714	-0.058453	4.816037
285.933156	8000.036372	14.135719	-0.058469	4.816031
286.189205	8000.043176	14.140723	-0.058517	4.816031
285.979152	8000.029745	14.145728	-0.058478	4.816029
285.999578	8000.050428	14.150733	-0.058481	4.816035
285.990633	8000.049204	14.155738	-0.058480	4.816034
285.923517	8000.036236	14.160743	-0.058467	4.816031
285.896549	8000.072086	14.165747	-0.058463	4.816041
285.994288	8000.032197	14.170752	-0.058481	4.816029
285.891248	8000.073074	14.175757	-0.058462	4.816042
285.946979	8000.051655	14.180762	-0.058472	4.816035
285.870866	8000.019289	14.185767	-0.058458	4.816026
285.856428	7999.978428	14.190771	-0.058455	4.816014
285.750394	7999.991467	14.195776	-0.058436	4.816019
285.690920	8000.010696	14.200781	-0.058425	4.816025
286.025125	8000.030676	14.205786	-0.058487	4.816029
285.909893	8000.014696	14.210791	-0.058466	4.816025
285.846029	8000.090480	14.215795	-0.058454	4.816047
285.925801	8000.056676	14.220800	-0.058469	4.816037
285.974934	8000.004148	14.225805	-0.058478	4.816021
285.878357	7999.441401	14.230810	-0.058460	4.815857

285.878994	7996.073698	14.235815	-0.058458	4.814873
285.715318	7990.616776	14.240819	-0.058424	4.813279
285.810415	7983.951416	14.245824	-0.058437	4.811330
285.745540	7976.636058	14.250829	-0.058421	4.809190
285.701351	7969.061968	14.255834	-0.058407	4.806974
285.580199	7961.208627	14.260839	-0.058380	4.804675
285.634452	7953.405776	14.265843	-0.058385	4.802389
285.461349	7945.365294	14.270848	-0.058348	4.800034
285.527357	7937.414785	14.275853	-0.058355	4.797702
285.448506	7929.437010	14.280858	-0.058335	4.795362
285.498517	7921.401458	14.285863	-0.058339	4.793003
285.457948	7913.384338	14.290867	-0.058326	4.790650
285.424432	7905.418042	14.295872	-0.058315	4.788309
285.249583	7897.367431	14.300877	-0.058277	4.785944
285.289130	7889.469604	14.305882	-0.058280	4.783621
285.405348	7881.395375	14.310887	-0.058296	4.781245
285.289366	7873.479605	14.315891	-0.058269	4.778915
285.303045	7865.435086	14.320896	-0.058267	4.776546
285.427558	7857.431148	14.325901	-0.058285	4.774187
285.318704	7849.380097	14.330906	-0.058259	4.771814
284.983984	7841.331983	14.335911	-0.058192	4.769441
285.185290	7833.408753	14.340915	-0.058224	4.767102
285.044711	7825.379923	14.345920	-0.058193	4.764733
284.791485	7817.446586	14.350925	-0.058141	4.762390
284.947064	7809.391835	14.355930	-0.058165	4.760009
284.823219	7801.447115	14.360935	-0.058136	4.757660
284.881965	7793.355793	14.365939	-0.058142	4.755266
284.820824	7785.362940	14.370944	-0.058126	4.752901
284.806005	7777.309342	14.375949	-0.058118	4.750516
284.669024	7769.367827	14.380954	-0.058087	4.748163
284.699257	7761.309184	14.385959	-0.058088	4.745774
284.934710	7753.352862	14.390963	-0.058126	4.743414
284.670778	7745.379712	14.395968	-0.058072	4.741049
284.769604	7737.371818	14.400973	-0.058085	4.738671
284.498965	7729.376243	14.405978	-0.058030	4.736297
284.344938	7721.342007	14.410983	-0.057996	4.733910
284.218314	7713.293303	14.415987	-0.057967	4.731518
284.147267	7705.278716	14.420992	-0.057949	4.729134
284.246232	7697.291016	14.425997	-0.057962	4.726756
284.304623	7689.308972	14.431002	-0.057968	4.724379
284.062767	7681.338283	14.436007	-0.057918	4.722005
284.083630	7673.329362	14.441011	-0.057916	4.719617
284.048772	7665.364751	14.446016	-0.057905	4.717242
284.027310	7657.322715	14.451021	-0.057896	4.714843
284.045949	7649.313404	14.456026	-0.057894	4.712451
284.169912	7641.256905	14.461031	-0.057912	4.710045
284.029520	7633.324242	14.466035	-0.057881	4.707674
283.945556	7625.242693	14.471040	-0.057860	4.705258
283.892054	7617.342977	14.476045	-0.057845	4.702895
283.922301	7609.355172	14.481050	-0.057845	4.700504
283.867545	7601.326933	14.486055	-0.057830	4.698101
283.966871	7593.325982	14.491059	-0.057843	4.695703
283.685371	7585.319769	14.496064	-0.057786	4.693304
283.683027	7577.234628	14.501069	-0.057780	4.690879
283.682168	7569.324273	14.506074	-0.057775	4.688505
283.620757	7561.274012	14.511079	-0.057758	4.686089
283.771722	7553.332352	14.516083	-0.057781	4.683703
283.543772	7545.288148	14.521088	-0.057734	4.681286
283.570551	7537.325726	14.526093	-0.057734	4.678891
283.387934	7529.316176	14.531098	-0.057695	4.676482
283.168679	7521.175793	14.536103	-0.057648	4.674032
283.223098	7513.190738	14.541107	-0.057653	4.671628
283.237605	7505.194000	14.546112	-0.057651	4.669218
283.318207	7497.213172	14.551117	-0.057661	4.666812
283.279233	7489.241962	14.556122	-0.057649	4.664408
283.071787	7481.290504	14.561127	-0.057605	4.662008
283.103923	7473.249402	14.566131	-0.057606	4.659580
283.016542	7465.238736	14.571136	-0.057584	4.657160
282.970657	7457.258297	14.576141	-0.057571	4.654748
282.942860	7449.274882	14.581146	-0.057560	4.652334
282.730878	7441.159660	14.586151	-0.057516	4.649879
282.793581	7433.247963	14.591155	-0.057522	4.647484
282.810635	7425.189689	14.596160	-0.057520	4.645043
282.673012	7417.266872	14.601165	-0.057490	4.642642
282.746196	7409.234745	14.606170	-0.057498	4.640207
282.632924	7401.248333	14.611175	-0.057472	4.637784
282.795777	7393.225945	14.616179	-0.057497	4.635349
282.570848	7385.232180	14.621184	-0.057450	4.632922
282.591804	7377.159201	14.626189	-0.057449	4.630469
282.533716	7369.207322	14.631194	-0.057433	4.628051
282.316564	7361.177125	14.636199	-0.057387	4.625609
282.440422	7353.233101	14.641203	-0.057405	4.623191
282.440176	7345.192464	14.646208	-0.057400	4.620743
282.281457	7337.203931	14.651213	-0.057365	4.618309
282.275677	7329.202549	14.656218	-0.057359	4.615870
282.249537	7321.179787	14.661223	-0.057349	4.613424
282.361829	7313.164566	14.666227	-0.057365	4.610978
282.185644	7305.196147	14.671232	-0.057327	4.608545
282.008768	7297.170704	14.676237	-0.057289	4.606094
282.124453	7289.226448	14.681242	-0.057305	4.603666
282.074294	7281.164776	14.686247	-0.057291	4.601201
282.101695	7273.204402	14.691251	-0.057291	4.598765
281.680703	7265.178799	14.696256	-0.057207	4.596309
281.820977	7257.140364	14.701261	-0.057228	4.593847
281.747580	7249.138815	14.706266	-0.057209	4.591395
281.741414	7241.120177	14.711271	-0.057203	4.588936
281.719023	7233.096699	14.716275	-0.057194	4.586475
281.600543	7225.138629	14.721280	-0.057167	4.584032
281.684206	7217.121655	14.726285	-0.057177	4.581570
281.642641	7209.149737	14.731290	-0.057164	4.579120
281.471474	7201.132535	14.736295	-0.057127	4.576656
281.532940	7193.154888	14.741299	-0.057133	4.574202
281.536706	7185.120757	14.746304	-0.057129	4.571729
281.313350	7177.096480	14.751309	-0.057082	4.569258
281.160303	7169.171718	14.756314	-0.057049	4.566816
281.066943	7161.154938	14.761319	-0.057026	4.564345
281.320031	7153.190255	14.766323	-0.057068	4.561888
281.020066	7145.167539	14.771328	-0.057007	4.559412
280.882889	7137.161979	14.776333	-0.056976	4.556940
280.827408	7129.109050	14.781338	-0.056961	4.554453
280.803100	7121.086701	14.786343	-0.056951	4.551973
280.851277	7113.073537	14.791347	-0.056955	4.549494
280.803473	7105.132658	14.796352	-0.056941	4.547037
280.714798	7097.072263	14.801357	-0.056919	4.544541
280.739832	7089.204285	14.806362	-0.056919	4.542104
280.558947	7081.133966	14.811367	-0.056880	4.539602
280.679920	7073.153384	14.816371	-0.056898	4.537128
280.477029	7065.165545	14.821376	-0.056855	4.534649
280.586735	7057.103240	14.826381	-0.056870	4.532146
280.700448	7049.093563	14.831386	-0.056886	4.529658
280.508168	7041.112946	14.836391	-0.056845	4.527177
280.333184	7033.115616	14.841395	-0.056807	4.524690
280.336783	7025.136805	14.846400	-0.056803	4.522207
280.454612	7017.051438	14.851405	-0.056820	4.519690
280.453427	7009.181669	14.856410	-0.056814	4.517239
280.385041	7001.088269	14.861415	-0.056796	4.514716
280.355078	6993.057233	14.866419	-0.056786	4.512212
280.360378	6985.071457	14.871424	-0.056782	4.509720
280.241337	6977.078947	14.876429	-0.056754	4.507225
280.228385	6969.098171	14.881434	-0.056747	4.504732
280.113329	6961.082613	14.886439	-0.056720	4.502226
280.248234	6953.058748	14.891443	-0.056740	4.499718
280.326348	6945.092613	14.896448	-0.056750	4.497225
280.158564	6937.066980	14.901453	-0.056713	4.494712
280.101455	6929.059975	14.906458	-0.056697	4.492204
279.940779	6921.054334	14.911463	-0.056662	4.489695
280.029322	6913.065093	14.916467	-0.056674	4.487190
279.729120	6905.057747	14.921472	-0.056613	4.484676
279.569137	6897.078645	14.926477	-0.056578	4.482171
279.876763	6889.100889	14.931482	-0.056630	4.479666
279.797567	6881.094272	14.936487	-0.056610	4.477149
279.809798	6873.036756	14.941491	-0.056607	4.474615
279.759453	6865.050863	14.946496	-0.056593	4.472103
279.791295	6857.033990	14.951501	-0.056594	4.469579
279.826333	6849.047370	14.956506	-0.056595	4.467063
279.550990	6841.025801	14.961511	-0.056539	4.464534
279.643679	6833.072401	14.966515	-0.056551	4.462026
279.585193	6825.046889	14.971520	-0.056535	4.459493
279.413928	6817.035083	14.976525	-0.056498	4.456963
279.511912	6809.035838	14.981530	-0.056511	4.454437
279.223008	6800.989106	14.986535	-0.056452	4.451892
279.236850	6793.017697	14.991539	-0.056449	4.449371
279.096153	6785.015103	14.996544	-0.056418	4.446838
279.029222	6777.007399	15.001549	-0.056400	4.444303
279.107425	6769.098140	15.006554	-0.056410	4.441797
278.973111	6761.000930	15.011559	-0.056380	4.439230
279.059866	6753.028760	15.016563	-0.056391	4.436702
279.009071	6744.984143	15.021568	-0.056376	4.434149
278.827508	6736.965501	15.026573	-0.056337	4.431602
278.778970	6728.987169	15.031578	-0.056323	4.429067
278.681660	6720.946325	15.036583	-0.056300	4.426510
278.738037	6712.985655	15.041587	-0.056305	4.423978
278.672619	6705.009590	15.046592	-0.056288	4.421439
278.498681	6696.968073	15.051597	-0.056250	4.418878
278.640488	6689.008231	15.056602	-0.056271	4.416342
278.367562	6680.954959	15.061607	-0.056215	4.413773
278.793352	6672.967001	15.066611	-0.056290	4.411227
278.680189	6664.994195	15.071616	-0.056263	4.408682
278.440016	6656.954608	15.076621	-0.056214	4.406113
278.307797	6649.007092	15.081626	-0.056184	4.403572
278.164092	6641.002902	15.086631	-0.056152	4.401012
278.202425	6633.055297	15.091635	-0.056154	4.398470
278.179481	6625.017678	15.096640	-0.056145	4.395897
278.112532	6616.977673	15.101645	-0.056127	4.393321
278.031316	6608.949460	15.106650	-0.056107	4.390747
277.792157	6600.956741	15.111655	-0.056057	4.388183
277.906002	6592.954335	15.116659	-0.056073	4.385616
277.975822	6584.977713	15.121664	-0.056081	4.383055
277.826149	6576.964676	15.126669	-0.056048	4.380480
277.954887	6568.988651	15.131674	-0.056067	4.377917
277.997219	6560.983784	15.136679	-0.056070	4.375343
277.958407	6552.981131	15.141683	-0.056057	4.372767
277.836625	6544.963333	15.146688	-0.056029	4.370184
277.782170	6536.984022	15.151693	-0.056014	4.367613
277.851871	6528.996589	15.156698	-0.056022	4.365038
277.601330	6521.126984	15.161703	-0.055970	4.362498
277.463669	6513.020222	15.166707	-0.055939	4.359881
277.403914	6505.028096	15.171712	-0.055923	4.357299
277.311459	6496.909998	15.176717	-0.055901	4.354675
277.152726	6488.895564	15.181722	-0.055866	4.352083
277.273857	6480.840172	15.186727	-0.055883	4.349477
277.184812	6472.930475	15.191731	-0.055862	4.346916
277.037977	6464.952410	15.196736	-0.055829	4.344330
277.079094	6456.972610	15.201741	-0.055832	4.341744
277.056783	6448.948764	15.206746	-0.055823	4.339142
277.041774	6440.964226	15.211751	-0.055815	4.336550
277.087156	6432.993835	15.216755	-0.055818	4.333963
276.924473	6424.940196	15.221760	-0.055782	4.331345
276.799017	6416.969457	15.226765	-0.055754	4.328753
276.614234	6408.979832	15.231770	-0.055714	4.326152
276.595188	6400.943694	15.236775	-0.055706	4.323536
276.618430	6392.944126	15.241779	-0.055705	4.320931
276.441030	6384.978544	15.246784	-0.055667	4.318334
276.392240	6376.937551	15.251789	-0.055653	4.315711
276.525497	6368.950141	15.256794	-0.055672	4.313106
276.430467	6360.901758	15.261799	-0.055649	4.310478
276.414101	6352.960730	15.266803	-0.055641	4.307883
276.439876	6344.910900	15.271808	-0.055641	4.305252
276.329534	6336.940606	15.276813	-0.055615	4.302644
276.315394	6328.947272	15.281818	-0.055607	4.300028
276.290771	6320.962868	15.286823	-0.055598	4.297413
276.266156	6312.930957	15.291827	-0.055588	4.294781
276.071332	6304.906034	15.296832	-0.055547	4.292148
276.217123	6296.878151	15.301837	-0.055569	4.289515
276.267809	6288.926790	15.306842	-0.055573	4.286905
276.093737	6280.908647	15.311847	-0.055535	4.284270
276.120915	6272.914427	15.316851	-0.055535	4.281643
276.222916	6264.965054	15.321856	-0.055549	4.279029
276.108333	6256.896809	15.326861	-0.055523	4.276373
276.063260	6248.923855	15.331866	-0.055509	4.273747
275.853984	6240.896434	15.336871	-0.055465	4.271100
275.925501	6232.891684	15.341875	-0.055473	4.268461
275.909094	6224.872317	15.346880	-0.055465	4.265815
275.635262	6216.875811	15.351885	-0.055409	4.263173
275.715778	6208.904617	15.356890	-0.055419	4.260541
275.501642	6200.910974	15.361895	-0.055374	4.257897
275.454003	6192.900144	15.366899	-0.055360	4.255247
275.495895	6184.878788	15.371904	-0.055362	4.252592
275.364177	6176.855693	15.376909	-0.055333	4.249934
275.491237	6168.925000	15.381914	-0.055351	4.247307
275.331437	6160.871291	15.386919	-0.055316	4.244636
275.489758	6152.968436	15.391923	-0.055341	4.242015
275.321249	6144.970216	15.396928	-0.055304	4.239358
275.197163	6136.944869	15.401933	-0.055276	4.236691
275.341522	6128.951992	15.406938	-0.055298	4.234035
275.113189	6120.874938	15.411943	-0.055250	4.231347
275.107516	6112.902872	15.416947	-0.055244	4.228693
275.164862	6104.875010	15.421952	-0.055249	4.226020
275.026393	6096.909259	15.426957	-0.055219	4.223364
274.838223	6088.921919	15.431962	-0.055178	4.220699
274.800970	6080.960637	15.436967	-0.055166	4.218042
274.914449	6072.928066	15.441971	-0.055182	4.215361
274.783907	6064.950629	15.446976	-0.055153	4.212695
274.959783	6056.867581	15.451981	-0.055181	4.209994
274.832743	6048.959980	15.456986	-0.055152	4.207348
274.717488	6040.919073	15.461991	-0.055125	4.204655
274.639725	6032.959590	15.466995	-0.055106	4.201988
274.621214	6024.972690	15.472000	-0.055097	4.199311
274.609932	6016.941359	15.477005	-0.055090	4.196618
274.577025	6008.875866	15.482010	-0.055078	4.193911
274.433030	6000.819933	15.487015	-0.055046	4.191204
274.481765	5992.871999	15.492019	-0.055050	4.188533
274.290013	5984.882744	15.497024	-0.055010	4.185845
274.216573	5976.885740	15.502029	-0.054991	4.183154
274.312932	5968.901565	15.507034	-0.055004	4.180467
274.244850	5960.886001	15.512039	-0.054986	4.177765
274.043395	5952.891932	15.517043	-0.054943	4.175068
274.085036	5944.897193	15.522048	-0.054946	4.172372
274.050992	5936.864744	15.527053	-0.054934	4.169660
273.951329	5928.934837	15.532058	-0.054911	4.166980
273.949347	5920.888704	15.537063	-0.054905	4.164261
274.004105	5912.918875	15.542067	-0.054910	4.161566
273.880092	5904.925045	15.547072	-0.054882	4.158859
273.757440	5896.908785	15.552077	-0.054854	4.156143
273.815917	5888.879809	15.557082	-0.054860	4.153423
273.875665	5880.861556	15.562087	-0.054866	4.150704
273.799698	5872.860476	15.567091	-0.054846	4.147989
273.838905	5864.872716	15.572096	-0.054849	4.145277
273.656984	5856.911501	15.577101	-0.054810	4.142570
273.615027	5848.916802	15.582106	-0.054797	4.139851
273.505966	5840.894839	15.587111	-0.054771	4.137121
273.515559	5832.864936	15.592115	-0.054768	4.134387
273.493516	5824.846949	15.597120	-0.054759	4.131655
273.168187	5816.892539	15.602125	-0.054693	4.128940
273.462366	5808.842030	15.607130	-0.054743	4.126197
273.343011	5800.901959	15.612135	-0.054715	4.123485
273.279393	5792.905788	15.617139	-0.054698	4.120753
273.321888	5784.929406	15.622144	-0.054701	4.118027
273.317112	5776.880615	15.627149	-0.054695	4.115274
273.125997	5768.881368	15.632154	-0.054654	4.112534
273.003369	5760.865905	15.637159	-0.054626	4.109788
273.042613	5752.882704	15.642163	-0.054629	4.107052
272.834918	5744.874787	15.647168	-0.054585	4.104303
272.783708	5736.866528	15.652173	-0.054570	4.101554
272.865973	5728.919583	15.657178	-0.054580	4.098826
272.702435	5720.900830	15.662183	-0.054545	4.096068
272.616851	5712.915475	15.667187	-0.054524	4.093321
272.544645	5704.887854	15.672192	-0.054505	4.090558
272.545867	5696.891905	15.677197	-0.054500	4.087805
272.461839	5688.903705	15.682202	-0.054479	4.085051
272.259312	5680.946306	15.687207	-0.054437	4.082305
272.351178	5672.928709	15.692211	-0.054448	4.079540
272.338425	5664.965774	15.697216	-0.054441	4.076790
272.519628	5656.857935	15.702221	-0.054470	4.073991
272.568976	5648.884437	15.707226	-0.054474	4.071235
272.374526	5640.925032	15.712231	-0.054432	4.068479
272.471411	5632.902778	15.717235	-0.054445	4.065703
272.376854	5624.951244	15.722240	-0.054422	4.062947
272.188359	5616.929690	15.727245	-0.054382	4.060163
272.249313	5608.971167	15.732250	-0.054388	4.057403
271.934300	5600.913661	15.737255	-0.054325	4.054601
271.893877	5592.929776	15.742259	-0.054312	4.051827
272.119200	5584.926181	15.747264	-0.054349	4.049048
271.895328	5576.899750	15.752269	-0.054302	4.046252
271.970240	5568.942869	15.757274	-0.054311	4.043483
271.904262	5560.924675	15.762279	-0.054293	4.040689
271.913480	5552.942061	15.767283	-0.054290	4.037907
271.788946	5544.947278	15.772288	-0.054262	4.035116
271.549371	5536.796626	15.777293	-0.054212	4.032267
271.612336	5528.847247	15.782298	-0.054218	4.029491
271.602489	5520.884984	15.787303	-0.054212	4.026707
271.625166	5512.867081	15.792307	-0.054211	4.023903
271.645445	5504.912817	15.797312	-0.054209	4.021119
271.472492	5496.926920	15.802317	-0.054172	4.018318
271.443276	5488.899517	15.807322	-0.054161	4.015504
271.266058	5480.889512	15.812327	-0.054123	4.012691
271.315534	5472.849558	15.817331	-0.054127	4.009870
271.350861	5464.937579	15.822336	-0.054129	4.007091
271.346040	5456.864165	15.827341	-0.054123	4.004253
271.353755	5448.959167	15.832346	-0.054119	4.001472
271.178134	5440.941900	15.837351	-0.054081	3.998647
271.134752	5432.920069	15.842355	-0.054068	3.995820
271.168770	5424.873037	15.847360	-0.054069	3.992984
270.962553	5416.854883	15.852365	-0.054026	3.990152
270.902424	5408.917258	15.857370	-0.054009	3.987348
270.897905	5400.869658	15.862375	-0.054003	3.984505
270.925714	5392.919913	15.867379	-0.054003	3.981695
270.815619	5384.953843	15.872384	-0.053978	3.978875
270.939403	5376.911349	15.877389	-0.053996	3.976030
270.833994	5368.923880	15.882394	-0.053971	3.973198
270.583088	5360.874066	15.887399	-0.053919	3.970340
270.585531	5352.903716	15.892403	-0.053914	3.967512
270.527396	5344.927816	15.897408	-0.053898	3.964679
270.492448	5336.966225	15.902413	-0.053887	3.961850
270.443706	5328.971495	15.907418	-0.053873	3.959006
270.445067	5320.973153	15.912423	-0.053868	3.956160
270.476782	5312.932684	15.917427	-0.053868	3.953297
270.395900	5304.899013	15.922432	-0.053848	3.950433
270.290348	5296.907397	15.927437	-0.053823	3.947582
270.237266	5288.940076	15.932442	-0.053808	3.944738
270.126991	5280.965558	15.937447	-0.053783	3.941888
270.119853	5272.977896	15.942451	-0.053776	3.939033
270.225545	5264.984445	15.947456	-0.053791	3.936176
270.162761	5256.936963	15.952461	-0.053774	3.933295
270.116855	5248.947737	15.957466	-0.053760	3.930433
270.036825	5240.977354	15.962471	-0.053740	3.927574
270.213778	5232.946183	15.967475	-0.053768	3.924697
270.006749	5225.025069	15.972480	-0.053725	3.921850
269.678717	5217.027205	15.977485	-0.053658	3.918971
269.779521	5208.993107	15.982490	-0.053672	3.916085
269.714571	5200.958461	15.987495	-0.053655	3.913193
269.541677	5192.940424	15.992499	-0.053617	3.910303
269.627148	5185.013221	15.997504	-0.053628	3.907449
269.434269	5176.971736	16.002509	-0.053587	3.904546
269.354369	5169.001492	16.007514	-0.053567	3.901669
269.450510	5160.982359	16.012519	-0.053580	3.898775
269.467941	5152.988732	16.017523	-0.053578	3.895887
269.372192	5144.980971	16.022528	-0.053555	3.892989
269.285857	5136.933028	16.027533	-0.053534	3.890075
269.408558	5128.982854	16.032538	-0.053552	3.887198
269.157510	5120.973607	16.037543	-0.053500	3.884291
269.121258	5113.003120	16.042547	-0.053488	3.881399
269.240908	5105.003757	16.047552	-0.053505	3.878498
269.226210	5096.983048	16.052557	-0.053497	3.875584
269.087213	5088.801542	16.057562	-0.053466	3.872607
269.035959	5080.790729	16.062567	-0.053451	3.869692
268.913536	5072.873779	16.067571	-0.053423	3.866807
269.158601	5064.926014	16.072576	-0.053464	3.863916
268.960680	5056.932552	16.077581	-0.053422	3.860998
268.977424	5048.978137	16.082586	-0.053420	3.858096
268.890161	5040.985762	16.087591	-0.053399	3.855175
268.716560	5032.982821	16.092595	-0.053361	3.852247
268.645302	5025.013754	16.097600	-0.053343	3.849331
268.654911	5016.956816	16.102605	-0.053339	3.846383
268.691179	5008.977868	16.107610	-0.053341	3.843461
268.283169	5001.023468	16.112615	-0.053260	3.840537
268.335078	4993.059267	16.117619	-0.053264	3.837616
268.241358	4985.055632	16.122624	-0.053242	3.834676
268.184039	4977.011140	16.127629	-0.053226	3.831719
268.221759	4969.006626	16.132634	-0.053228	3.828776
268.362648	4960.987212	16.137639	-0.053249	3.825828
268.153698	4953.046128	16.142643	-0.053205	3.822899
268.054724	4945.046596	16.147648	-0.053181	3.819949
268.109008	4937.070004	16.152653	-0.053186	3.817008
268.346437	4929.043487	16.157658	-0.053226	3.814050
268.075193	4921.033500	16.162663	-0.053170	3.811086
268.226617	4913.042845	16.167667	-0.053193	3.808135
268.118125	4905.060584	16.172672	-0.053168	3.805179
267.929472	4897.084136	16.177677	-0.053127	3.802222
268.043172	4889.100730	16.182682	-0.053143	3.799266
267.904403	4881.101098	16.187687	-0.053112	3.796296
267.883320	4873.047976	16.192691	-0.053103	3.793307
267.600915	4865.030749	16.197696	-0.053046	3.790323
267.543086	4857.042077	16.202701	-0.053030	3.787352
267.785571	4849.052971	16.207706	-0.053070	3.784385
267.504635	4841.072378	16.212711	-0.053012	3.781408
267.570618	4833.076849	16.217715	-0.053019	3.778430
267.459506	4825.072164	16.222720	-0.052994	3.775443
267.395186	4817.051852	16.227725	-0.052977	3.772448
267.487484	4809.097942	16.232730	-0.052989	3.769479
267.455776	4801.049156	16.237735	-0.052978	3.766470
267.263045	4793.084908	16.242739	-0.052937	3.763486
267.089031	4785.102598	16.247744	-0.052899	3.760494
267.200451	4777.096964	16.252749	-0.052915	3.757497
267.046086	4769.122127	16.257754	-0.052881	3.754503
267.074875	4761.064409	16.262759	-0.052881	3.751479
267.033363	4753.099731	16.267763	-0.052868	3.748487
267.047025	4745.052545	16.272768	-0.052866	3.745462
266.968698	4737.089684	16.277773	-0.052846	3.742465
266.912074	4729.123617	16.282778	-0.052830	3.739464
266.789174	4721.118381	16.287783	-0.052802	3.736445
266.976883	4713.090471	16.292787	-0.052832	3.733422
266.785251	4705.081852	16.297792	-0.052791	3.730395
266.794762	4697.090397	16.302797	-0.052788	3.727377
266.821484	4689.114245	16.307802	-0.052788	3.724362
266.452283	4681.164474	16.312807	-0.052714	3.721345
266.305133	4673.179301	16.317811	-0.052681	3.718318
266.488416	4665.173221	16.322816	-0.052710	3.715289
266.357613	4657.075853	16.327821	-0.052681	3.712214
266.303560	4649.101229	16.332826	-0.052666	3.709186
266.281454	4641.078535	16.337831	-0.052656	3.706138
266.348974	4633.137979	16.342835	-0.052664	3.703120
266.303476	4625.166840	16.347840	-0.052650	3.700086
266.072912	4617.165837	16.352845	-0.052602	3.697033
266.220834	4609.195411	16.357850	-0.052625	3.693999
266.089682	4601.160382	16.362855	-0.052595	3.690931
266.178474	4593.175026	16.367859	-0.052606	3.687884
266.190043	4585.171866	16.372864	-0.052603	3.684827
266.005282	4577.243675	16.377869	-0.052564	3.681790
266.042624	4569.242320	16.382874	-0.052566	3.678729
265.953225	4561.224176	16.387879	-0.052544	3.675655
265.991442	4553.219835	16.392883	-0.052546	3.672588
265.832672	4545.201041	16.397888	-0.052511	3.669507
265.792851	4537.172228	16.402893	-0.052499	3.666423
265.741446	4529.227289	16.407898	-0.052484	3.663368
265.553203	4521.200785	16.412903	-0.052444	3.660275
265.495474	4513.251045	16.417907	-0.052428	3.657213
265.551241	4505.247732	16.422912	-0.052433	3.654131
265.492584	4497.173889	16.427917	-0.052417	3.651016
265.571758	4489.234304	16.432922	-0.052427	3.647953
265.508556	4481.209209	16.437927	-0.052410	3.644852
265.478872	4473.285561	16.442931	-0.052399	3.641787
265.350570	4465.297089	16.447936	-0.052370	3.638693
265.364653	4457.249347	16.452941	-0.052368	3.635577
265.406448	4449.233175	16.457946	-0.052370	3.632470
265.096768	4441.216617	16.462951	-0.052307	3.629352
264.952609	4433.214981	16.467955	-0.052275	3.626241
265.160557	4425.257791	16.472960	-0.052309	3.623155
265.043315	4417.245576	16.477965	-0.052282	3.620035
264.850494	4409.329749	16.482970	-0.052241	3.616948
264.823538	4401.270653	16.487975	-0.052231	3.613808
264.831512	4393.261755	16.492979	-0.052227	3.610685
264.803016	4385.320710	16.497984	-0.052217	3.607585
264.610196	4377.284615	16.502989	-0.052176	3.604440
264.602081	4369.359145	16.507994	-0.052169	3.601341
264.499385	4361.345111	16.512999	-0.052145	3.598202
264.465975	4353.326043	16.518003	-0.052134	3.595061
264.489988	4345.337790	16.523008	-0.052133	3.591930
264.392791	4337.302295	16.528013	-0.052110	3.588775
264.320230	4329.330962	16.533018	-0.052091	3.585642
264.325747	4321.357867	16.538023	-0.052087	3.582509
264.331348	4313.360806	16.543027	-0.052083	3.579363
264.208728	4305.418055	16.548032	-0.052055	3.576232
264.066957	4297.355417	16.553037	-0.052023	3.573051
264.302318	4289.358176	16.558042	-0.052062	3.569903
264.111186	4281.401216	16.563047	-0.052021	3.566757
263.925445	4273.401222	16.568051	-0.051982	3.563590
263.915423	4265.436636	16.573056	-0.051975	3.560440
263.855509	4257.429939	16.578061	-0.051958	3.557269
263.808758	4249.390065	16.583066	-0.051945	3.554083
263.632632	4241.300056	16.588071	-0.051907	3.550869
263.677677	4233.358389	16.593075	-0.051910	3.547719
263.705766	4225.366101	16.598080	-0.051910	3.544545
263.478905	4217.407717	16.603085	-0.051863	3.541374
263.610034	4209.407216	16.608090	-0.051882	3.538193
263.528303	4201.391331	16.613095	-0.051862	3.534998
263.512049	4193.395847	16.618099	-0.051853	3.531810
263.549460	4185.397317	16.623104	-0.051855	3.528619
263.337146	4177.406802	16.628109	-0.051811	3.525421
263.292800	4169.473434	16.633114	-0.051797	3.522248
263.368126	4161.465675	16.638119	-0.051806	3.519046
263.441203	4153.494174	16.643123	-0.051815	3.515856
263.345957	4145.477267	16.648128	-0.051792	3.512640
263.127077	4137.446829	16.653133	-0.051746	3.509411
263.202827	4129.467455	16.658138	-0.051755	3.506209
263.026919	4121.487420	16.663143	-0.051717	3.502995
262.823565	4113.504488	16.668147	-0.051674	3.499777
263.029288	4105.539391	16.673152	-0.051707	3.496576
262.863522	4097.513361	16.678157	-0.051671	3.493336
262.849211	4089.501719	16.683162	-0.051663	3.490103
262.588343	4081.543657	16.688167	-0.051610	3.486881
262.731333	4073.530060	16.693171	-0.051631	3.483646
262.782848	4065.588814	16.698176	-0.051636	3.480435
262.669631	4057.579119	16.703181	-0.051609	3.477188
262.529252	4049.582938	16.708186	-0.051578	3.473942
262.598936	4041.547827	16.713191	-0.051586	3.470684
262.358603	4033.553832	16.718195	-0.051536	3.467430
262.468854	4025.575135	16.723200	-0.051551	3.464190
262.467751	4017.569705	16.728205	-0.051546	3.460933
262.413772	4009.618915	16.733210	-0.051531	3.457694
262.257907	4001.601023	16.738215	-0.051497	3.454420
262.160129	3993.581594	16.743219	-0.051473	3.451145
262.245185	3985.623240	16.748224	-0.051484	3.447897
262.214679	3977.575490	16.753229	-0.051473	3.444606
262.301647	3969.639657	16.758234	-0.051484	3.441362
262.190354	3961.641880	16.763239	-0.051459	3.438083
261.850028	3953.645889	16.768243	-0.051390	3.434793
262.016578	3945.622860	16.773248	-0.051416	3.431506
261.882494	3937.631788	16.778253	-0.051386	3.428220
261.914814	3929.643290	16.783258	-0.051387	3.424936
261.808160	3921.697254	16.788263	-0.051362	3.421662
261.756550	3913.698333	16.793267	-0.051347	3.418366
261.839579	3905.697664	16.798272	-0.051357	3.415069
261.561326	3897.684394	16.803277	-0.051300	3.411753
261.573852	3889.707281	16.808282	-0.051298	3.408457
261.405815	3881.686348	16.813287	-0.051261	3.405135
261.414044	3873.739438	16.818291	-0.051258	3.401845
261.345038	3865.777988	16.823296	-0.051240	3.398544
261.318756	3857.750798	16.828301	-0.051230	3.395214
261.308470	3849.674551	16.833306	-0.051223	3.391860
261.176174	3841.696810	16.838311	-0.051193	3.388541
261.215274	3833.687136	16.843315	-0.051195	3.385210
261.203939	3825.790721	16.848320	-0.051188	3.381922
261.095990	3817.765609	16.853325	-0.051163	3.378573
261.179917	3809.770518	16.858330	-0.051173	3.375240
260.960741	3801.794640	16.863335	-0.051127	3.371902
260.760009	3793.796100	16.868339	-0.051085	3.368551
260.947453	3785.798848	16.873344	-0.051114	3.365211
261.036099	3777.817836	16.878349	-0.051126	3.361871
260.816223	3769.847148	16.883354	-0.051080	3.358521
260.591036	3761.859697	16.888359	-0.051033	3.355160
260.753466	3753.823468	16.893363	-0.051058	3.351790
260.844853	3745.845111	16.898368	-0.051070	3.348438
260.603093	3737.832146	16.903373	-0.051019	3.345056
260.691670	3729.878212	16.908378	-0.051031	3.341707
260.616624	3721.876050	16.913383	-0.051012	3.338329
260.274814	3713.899912	16.918387	-0.050943	3.334948
260.376086	3705.919484	16.923392	-0.050957	3.331579
260.376436	3697.880626	16.928397	-0.050952	3.328177
260.203751	3689.900409	16.933402	-0.050914	3.324791
260.280825	3681.947105	16.938407	-0.050924	3.321422
260.156927	3673.950296	16.943411	-0.050895	3.318023
260.366687	3665.924435	16.948416	-0.050929	3.314621
259.995538	3657.947448	16.953421	-0.050855	3.311214
260.094093	3649.957311	16.958426	-0.050868	3.307816
259.991336	3641.975521	16.963431	-0.050844	3.304411
259.865747	3633.990134	16.968435	-0.050816	3.301000
259.841993	3626.026697	16.973440	-0.050806	3.297598
259.844521	3618.002008	16.978445	-0.050801	3.294167
259.964516	3610.001479	16.983450	-0.050819	3.290748
259.651374	3602.015782	16.988455	-0.050755	3.287315
259.627798	3594.009069	16.993459	-0.050746	3.283881
259.630161	3586.068754	16.998464	-0.050741	3.280472
259.363588	3578.116538	17.003469	-0.050686	3.277044
259.389963	3570.089851	17.008474	-0.050686	3.273592
259.452768	3562.051672	17.013479	-0.050692	3.270133
259.416530	3554.084480	17.018483	-0.050681	3.266697
259.493240	3546.093053	17.023488	-0.050690	3.263251
259.239133	3538.104654	17.028493	-0.050637	3.259790
259.569398	3530.148218	17.033498	-0.050694	3.256362
259.505396	3522.111957	17.038503	-0.050677	3.252881
259.373927	3514.114973	17.043507	-0.050647	3.249410
259.427147	3506.150698	17.048512	-0.050652	3.245956
259.266501	3498.181437	17.053517	-0.050617	3.242489
259.081988	3490.212212	17.058522	-0.050577	3.239017
259.178278	3482.217883	17.063527	-0.050590	3.235541
258.849775	3474.167463	17.068531	-0.050524	3.232020
258.819749	3466.177066	17.073536	-0.050513	3.228533
258.793976	3458.139190	17.078541	-0.050503	3.225022
258.720169	3450.202338	17.083546	-0.050484	3.221550
258.735382	3442.235853	17.088551	-0.050482	3.218064
258.594589	3434.245536	17.093555	-0.050451	3.214558
258.817813	3426.197979	17.098560	-0.050487	3.211037
258.799616	3418.233626	17.103565	-0.050479	3.207540
258.605722	3410.287360	17.108570	-0.050437	3.204039
258.411519	3402.317288	17.113575	-0.050396	3.200524
258.327922	3394.340690	17.118579	-0.050375	3.197007
258.412217	3386.330175	17.123584	-0.050386	3.193477
258.160071	3378.290340	17.128589	-0.050334	3.189917
258.154447	3370.311775	17.133594	-0.050328	3.186391
258.381874	3362.343178	17.138599	-0.050365	3.182875
258.120180	3354.374194	17.143603	-0.050311	3.179334
257.943272	3346.410355	17.148608	-0.050273	3.175794
257.761625	3338.370895	17.153613	-0.050234	3.172218
257.838518	3330.386737	17.158618	-0.050243	3.168672
257.785305	3322.404332	17.163623	-0.050228	3.165118
257.939982	3314.420035	17.168627	-0.050252	3.161568
257.712707	3306.475143	17.173632	-0.050205	3.158015
257.676594	3298.442575	17.178637	-0.050193	3.154427
257.893284	3290.412855	17.183642	-0.050228	3.150848
257.834573	3282.429315	17.188647	-0.050212	3.147273
257.619932	3274.452616	17.193651	-0.050167	3.143690
257.689357	3266.491557	17.198656	-0.050175	3.140122
257.702458	3258.499838	17.203661	-0.050172	3.136535
257.658693	3250.520041	17.208666	-0.050159	3.132946
257.552432	3242.491748	17.213671	-0.050134	3.129328
257.360074	3234.540800	17.218675	-0.050093	3.125737
257.377537	3226.597826	17.223680	-0.050091	3.122155
257.109617	3218.640948	17.228685	-0.050036	3.118549
257.310015	3210.603016	17.233690	-0.050068	3.114924
257.208726	3202.606248	17.238695	-0.050044	3.111300
256.981713	3194.623738	17.243699	-0.049997	3.107672
257.015564	3186.654335	17.248704	-0.049998	3.104058
257.063931	3178.639178	17.253709	-0.050002	3.100419
256.866577	3170.708673	17.258714	-0.049960	3.096803
256.901475	3162.679361	17.263719	-0.049961	3.093149
256.902934	3154.638228	17.268723	-0.049956	3.089484
256.964757	3146.693564	17.273728	-0.049963	3.085860
256.678897	3138.735088	17.278733	-0.049904	3.082211
256.624395	3130.761534	17.283738	-0.049889	3.078561
256.646272	3122.770009	17.288743	-0.049888	3.074901
256.330243	3114.711228	17.293747	-0.049824	3.071191
256.418622	3106.738972	17.298752	-0.049835	3.067535
256.524391	3098.716040	17.303757	-0.049850	3.063852
256.391621	3090.776437	17.308762	-0.049820	3.060192
256.251567	3082.814642	17.313767	-0.049789	3.056516
256.246376	3074.809512	17.318771	-0.049783	3.052823
256.420253	3066.818737	17.323776	-0.049810	3.049140
256.319886	3058.812990	17.328781	-0.049786	3.045433
256.249373	3050.892822	17.333786	-0.049768	3.041763
256.201637	3042.909914	17.338791	-0.049754	3.038060
256.081881	3034.919984	17.343795	-0.049727	3.034346
255.707858	3026.940624	17.348800	-0.049652	3.030619
255.938285	3018.923536	17.353805	-0.049690	3.026900
255.937461	3010.958220	17.358810	-0.049684	3.023189
255.908138	3002.961495	17.363815	-0.049674	3.019458
255.920000	2994.987092	17.368819	-0.049671	3.015734
255.861576	2987.003832	17.373824	-0.049655	3.011999
255.485437	2979.030342	17.378829	-0.049580	3.008247
255.549147	2971.040311	17.383834	-0.049586	3.004505
255.710379	2963.054643	17.388839	-0.049611	3.000765
255.478762	2955.100155	17.393843	-0.049563	2.997015
255.492816	2947.090794	17.398848	-0.049561	2.993247
255.522601	2939.055418	17.403853	-0.049561	2.989463
255.327497	2931.095603	17.408858	-0.049520	2.985699
255.382038	2923.128125	17.413863	-0.049525	2.981938
255.239344	2915.164510	17.418867	-0.049493	2.978165
255.354468	2907.185685	17.423872	-0.049509	2.974392
255.278330	2899.158945	17.428877	-0.049490	2.970583
255.097528	2891.214810	17.433882	-0.049451	2.966803
255.100442	2883.221913	17.438887	-0.049447	2.963003
255.071224	2875.240079	17.443891	-0.049436	2.959203
255.026198	2867.291159	17.448896	-0.049423	2.955413
254.823997	2859.278437	17.453901	-0.049380	2.951579
254.951378	2851.300889	17.458906	-0.049398	2.947774
254.840338	2843.312943	17.463911	-0.049373	2.943946
254.718967	2835.342420	17.468915	-0.049345	2.940122
254.749814	2827.385399	17.473920	-0.049345	2.936307
254.593323	2819.366740	17.478925	-0.049311	2.932447
254.716519	2811.387426	17.483930	-0.049329	2.928616
254.614686	2803.396287	17.488935	-0.049305	2.924763
254.517590	2795.436572	17.493939	-0.049282	2.920920
254.540099	2787.481452	17.498944	-0.049281	2.917080
254.519503	2779.401468	17.503949	-0.049272	2.913173
254.509719	2771.384000	17.508954	-0.049265	2.909291
254.305979	2763.436469	17.513959	-0.049222	2.905427
254.194071	2755.486964	17.518963	-0.049196	2.901562
254.378013	2747.509791	17.523968	-0.049225	2.897695
254.061809	2739.523284	17.528973	-0.049161	2.893791
254.131489	2731.526893	17.533978	-0.049169	2.889897
254.065930	2723.576014	17.538983	-0.049152	2.886014
253.996488	2715.612043	17.543987	-0.049133	2.882118
254.004459	2707.671326	17.548992	-0.049130	2.878233
253.679224	2699.652941	17.553997	-0.049064	2.874286
253.841943	2691.631463	17.559002	-0.049089	2.870359
253.754314	2683.669120	17.564007	-0.049068	2.866441
253.687219	2675.685613	17.569011	-0.049050	2.862510
253.679749	2667.725433	17.574016	-0.049044	2.858587
253.478426	2659.753658	17.579021	-0.049001	2.854643
253.328238	2651.782847	17.584026	-0.048968	2.850696
253.482302	2643.793962	17.589031	-0.048992	2.846752
253.373690	2635.816078	17.594035	-0.048966	2.842794
253.355678	2627.873721	17.599040	-0.048958	2.838852
253.353777	2619.841995	17.604045	-0.048952	2.834861
253.477041	2611.820565	17.609050	-0.048970	2.830877
253.155634	2603.883371	17.614055	-0.048905	2.826905
253.037883	2595.911847	17.619059	-0.048878	2.822921
253.074715	2587.951516	17.624064	-0.048880	2.818945
253.061804	2579.951329	17.629069	-0.048872	2.814942
252.920629	2571.965359	17.634074	-0.048841	2.810932
252.875088	2563.999186	17.639079	-0.048827	2.806932
252.762850	2556.009203	17.644083	-0.048801	2.802911
252.712349	2548.067673	17.649088	-0.048787	2.798912
252.584786	2540.092529	17.654093	-0.048758	2.794885
252.785352	2532.058985	17.659098	-0.048790	2.790842
252.587863	2524.106996	17.664103	-0.048748	2.786812
252.357101	2516.140266	17.669107	-0.048700	2.782766
252.488520	2508.176531	17.674112	-0.048720	2.778737
252.371038	2500.188007	17.679117	-0.048693	2.774675
252.279882	2492.200208	17.684122	-0.048671	2.770609
252.369727	2484.220883	17.689127	-0.048682	2.766552
252.328389	2476.251376	17.694131	-0.048669	2.762486
252.239478	2468.310789	17.699136	-0.048648	2.758426
252.183964	2460.304826	17.704141	-0.048632	2.754329
252.322742	2452.222246	17.709146	-0.048653	2.750198
252.427086	2444.269513	17.714151	-0.048667	2.746125
252.157575	2436.325713	17.719155	-0.048612	2.742029
252.051105	2428.402020	17.724160	-0.048587	2.737946
251.853396	2420.415591	17.729165	-0.048545	2.733819
251.968770	2412.388010	17.734170	-0.048561	2.729684
251.628907	2404.484363	17.739175	-0.048493	2.725579
251.544889	2396.508232	17.744179	-0.048472	2.721446
251.648063	2388.545506	17.749184	-0.048486	2.717325
251.611373	2380.542929	17.754189	-0.048474	2.713168
251.698604	2372.546871	17.759194	-0.048486	2.709016
251.668816	2364.570992	17.764199	-0.048475	2.704861
251.414619	2356.645574	17.769203	-0.048422	2.700712
251.413855	2348.678245	17.774208	-0.048417	2.696550
251.352451	2340.663103	17.779213	-0.048401	2.692354
251.454654	2332.686088	17.784218	-0.048415	2.688180
251.309318	2324.728591	17.789223	-0.048382	2.683995
251.158805	2316.775901	17.794227	-0.048349	2.679806
251.093988	2308.845536	17.799232	-0.048332	2.675627
250.935367	2300.814094	17.804237	-0.048297	2.671382
251.070874	2292.797697	17.809242	-0.048317	2.667158
250.920632	2284.857476	17.814247	-0.048284	2.662948
250.657995	2276.918226	17.819251	-0.048230	2.658726
250.621776	2268.960663	17.824256	-0.048219	2.654501
250.563269	2260.926349	17.829261	-0.048203	2.650227
250.530206	2252.988064	17.834266	-0.048191	2.645999
250.462607	2245.021361	17.839271	-0.048174	2.641747
250.339810	2237.061721	17.844275	-0.048146	2.637489
250.553149	2229.046371	17.849280	-0.048180	2.633215
250.405017	2221.057155	17.854285	-0.048147	2.628925
250.329368	2213.100049	17.859290	-0.048128	2.624650
250.398397	2205.147405	17.864295	-0.048136	2.620380
250.269932	2197.205112	17.869299	-0.048107	2.616095
250.234478	2189.216107	17.874304	-0.048095	2.611785
250.235886	2181.212067	17.879309	-0.048090	2.607461
250.151304	2173.284712	17.884314	-0.048070	2.603166
249.831965	2165.348129	17.889319	-0.048005	2.598843
250.169955	2157.302950	17.894323	-0.048063	2.594498
250.077719	2149.167179	17.899328	-0.048040	2.590068
249.735670	2141.259514	17.904333	-0.047972	2.585737
249.856723	2133.315994	17.909338	-0.047989	2.581411
249.885299	2125.371605	17.914343	-0.047989	2.577071
249.755854	2117.425062	17.919347	-0.047960	2.572712
249.632810	2109.468505	17.924352	-0.047932	2.568340
249.503173	2101.509644	17.929357	-0.047903	2.563959
249.695884	2093.534347	17.934362	-0.047934	2.559584
249.408988	2085.617502	17.939367	-0.047875	2.555200
249.381022	2077.607415	17.944371	-0.047865	2.550775
249.530938	2069.643714	17.949376	-0.047888	2.546380
249.342067	2061.692124	17.954381	-0.047847	2.541961
249.257711	2053.745140	17.959386	-0.047826	2.537544
249.035258	2045.784714	17.964391	-0.047780	2.533102
248.950905	2037.784401	17.969395	-0.047759	2.528640
249.033592	2029.829225	17.974400	-0.047769	2.524207
249.020208	2021.867033	17.979405	-0.047762	2.519755
249.070958	2013.904864	17.984410	-0.047766	2.515300
248.922712	2005.903016	17.989415	-0.047733	2.510801
248.771533	1997.953716	17.994419	-0.047700	2.506322
248.768823	1990.003237	17.999424	-0.047695	2.501846
248.661454	1982.029291	18.004429	-0.047669	2.497341
248.550437	1974.087378	18.009434	-0.047644	2.492846
248.549266	1966.093878	18.014439	-0.047638	2.488321
248.418729	1958.129981	18.019443	-0.047609	2.483795
248.312051	1950.213274	18.024448	-0.047584	2.479290
248.409727	1942.227254	18.029453	-0.047597	2.474752
248.347506	1934.250864	18.034458	-0.047580	2.470199
248.204784	1926.302953	18.039463	-0.047549	2.465649
248.052486	1918.343522	18.044467	-0.047515	2.461082
248.055804	1910.399875	18.049472	-0.047511	2.456528
247.953002	1902.416394	18.054477	-0.047486	2.451934
248.033569	1894.423134	18.059482	-0.047496	2.447340
248.025550	1886.477525	18.064487	-0.047490	2.442758
247.978205	1878.540103	18.069491	-0.047476	2.438169
247.895427	1870.561405	18.074496	-0.047455	2.433545
247.678461	1862.545381	18.079501	-0.047410	2.428880
247.576675	1854.608089	18.084506	-0.047386	2.424260
247.490594	1846.667566	18.089511	-0.047365	2.419632
247.529143	1838.688112	18.094515	-0.047367	2.414981
247.622930	1830.712682	18.099520	-0.047379	2.410328
247.320883	1822.775751	18.104525	-0.047318	2.405657
247.312881	1814.832933	18.109530	-0.047311	2.400997
247.220897	1806.894675	18.114535	-0.047289	2.396324
247.147158	1798.915767	18.119539	-0.047270	2.391619
247.217481	1790.937620	18.124544	-0.047278	2.386917
247.101624	1782.986282	18.129549	-0.047251	2.382207
247.050998	1775.050438	18.134554	-0.047237	2.377502
247.171106	1767.077516	18.139559	-0.047254	2.372778
246.876505	1759.131421	18.144563	-0.047194	2.368029
246.977906	1751.173914	18.149568	-0.047208	2.363294
246.881070	1743.229690	18.154573	-0.047185	2.358543
246.740446	1735.281105	18.159578	-0.047153	2.353775
246.684557	1727.307110	18.164583	-0.047138	2.348989
246.581200	1719.339712	18.169587	-0.047114	2.344194
246.731507	1711.383891	18.174592	-0.047136	2.339416
246.438240	1703.445879	18.179597	-0.047077	2.334603
246.481696	1695.471781	18.184602	-0.047080	2.329786
246.285371	1687.531519	18.189607	-0.047038	2.324960
246.315452	1679.576295	18.194611	-0.047039	2.320133
246.518515	1671.622744	18.199616	-0.047071	2.315312
246.250895	1663.670015	18.204621	-0.047016	2.310442
246.252537	1655.703818	18.209626	-0.047012	2.305575
246.380831	1647.749835	18.214631	-0.047030	2.300717
246.214296	1639.808974	18.219635	-0.046994	2.295831
246.046613	1631.881470	18.224640	-0.046958	2.290944
245.821604	1623.932799	18.229645	-0.046911	2.286027
246.010458	1615.966901	18.234650	-0.046941	2.281125
245.853841	1608.051474	18.239655	-0.046907	2.276214
245.620980	1600.048324	18.244659	-0.046858	2.271231
245.613347	1592.082447	18.249664	-0.046852	2.266280
245.426188	1584.143037	18.254669	-0.046812	2.261319
245.555253	1576.178350	18.259674	-0.046831	2.256359
245.446906	1568.236847	18.264679	-0.046805	2.251381
245.293305	1560.283194	18.269683	-0.046772	2.246381
245.199953	1552.368985	18.274688	-0.046749	2.241400
245.224856	1544.411128	18.279693	-0.046749	2.236391
245.371919	1536.431792	18.284698	-0.046771	2.231367
245.370785	1528.479921	18.289703	-0.046766	2.226337
245.150306	1520.554566	18.294707	-0.046720	2.221292
245.178878	1512.618595	18.299712	-0.046720	2.216252
245.215753	1504.646112	18.304717	-0.046722	2.211177
244.878407	1496.741778	18.309722	-0.046654	2.206101
244.867584	1488.811386	18.314727	-0.046647	2.201025
244.799729	1480.865498	18.319731	-0.046629	2.195923
244.877476	1472.892103	18.324736	-0.046638	2.190804
244.647154	1464.949577	18.329741	-0.046590	2.185665
244.579234	1457.022216	18.334746	-0.046573	2.180539
244.518841	1449.092716	18.339751	-0.046556	2.175400
244.465158	1441.109671	18.344755	-0.046541	2.170214
244.512021	1433.165001	18.349760	-0.046545	2.165051
244.485164	1425.227482	18.354765	-0.046535	2.159873
244.505120	1417.305671	18.359770	-0.046533	2.154697
244.371376	1409.359821	18.364775	-0.046503	2.149478
244.206069	1401.412218	18.369779	-0.046467	2.144243
244.342522	1393.485018	18.374784	-0.046488	2.139036
244.026185	1385.574045	18.379789	-0.046424	2.133785
244.173512	1377.608968	18.384794	-0.046446	2.128529
244.124838	1369.684294	18.389799	-0.046432	2.123268
243.909696	1361.776014	18.394803	-0.046387	2.117989
243.871668	1353.803855	18.399808	-0.046375	2.112671
243.760797	1345.820053	18.404813	-0.046349	2.107325
243.758896	1337.900412	18.409818	-0.046343	2.102019
243.639736	1329.979635	18.414823	-0.046316	2.096687
243.482621	1322.041738	18.419827	-0.046282	2.091326
243.606269	1314.097913	18.424832	-0.046300	2.085976
243.252875	1306.212961	18.429837	-0.046229	2.080604
243.424539	1298.255540	18.434842	-0.046256	2.075221
243.391713	1290.309191	18.439847	-0.046244	2.069811
243.315168	1282.368508	18.444851	-0.046225	2.064386
243.257481	1274.474244	18.449856	-0.046209	2.058981
243.296492	1266.512495	18.454861	-0.046211	2.053525
243.420239	1258.555373	18.459866	-0.046229	2.048066
243.274334	1250.670832	18.464871	-0.046197	2.042616
243.222345	1242.750352	18.469875	-0.046182	2.037135
243.334419	1234.789771	18.474880	-0.046198	2.031629
242.840158	1226.904174	18.479885	-0.046101	2.026098
242.763465	1218.976073	18.484890	-0.046082	2.020564
242.835168	1211.045388	18.489895	-0.046090	2.015029
242.543438	1203.124675	18.494899	-0.046031	2.009449
242.575776	1195.198225	18.499904	-0.046032	2.003882
242.587777	1187.273975	18.504909	-0.046029	1.998299
242.651850	1179.330145	18.509914	-0.046036	1.992692
242.734954	1171.382894	18.514919	-0.046046	1.987069
242.584834	1163.475159	18.519923	-0.046013	1.981433
242.574456	1155.574688	18.524928	-0.046006	1.975801
242.156976	1147.691302	18.529933	-0.045923	1.970122
242.232720	1139.758677	18.534938	-0.045932	1.964444
242.427331	1131.824416	18.539943	-0.045963	1.958761
242.315484	1123.887491	18.544947	-0.045937	1.953026
242.129974	1115.963631	18.549952	-0.045898	1.947276
241.939378	1108.055680	18.554957	-0.045857	1.941520
242.059492	1100.118437	18.559962	-0.045874	1.935760
241.982944	1092.208835	18.564967	-0.045855	1.929981
241.649392	1084.320754	18.569971	-0.045788	1.924172
241.717161	1076.413658	18.574976	-0.045795	1.918375
241.532908	1068.504898	18.579981	-0.045756	1.912532
241.571517	1060.561001	18.584986	-0.045758	1.906670
241.487939	1052.661010	18.589991	-0.045738	1.900809
241.309103	1044.769023	18.594995	-0.045699	1.894924
241.407771	1036.836359	18.600000	-0.045712	1.889023
241.307582	1028.936685	18.605005	-0.045689	1.883105
241.217449	1021.053509	18.610010	-0.045667	1.877181
241.107755	1013.137754	18.615015	-0.045641	1.871212
241.072227	1005.199876	18.620019	-0.045630	1.865216
241.054789	997.318093	18.625024	-0.045621	1.859246
240.856170	989.426942	18.630029	-0.045579	1.853227
240.746283	981.513630	18.635034	-0.045554	1.847183
240.882859	973.588712	18.640039	-0.045574	1.841138
240.677732	965.715683	18.645043	-0.045531	1.835074
240.730771	957.795554	18.650048	-0.045536	1.828983
240.647217	949.903966	18.655053	-0.045515	1.822878
240.593852	942.009665	18.660058	-0.045500	1.816754
240.571769	934.107706	18.665063	-0.045491	1.810607
240.536747	926.204996	18.670067	-0.045479	1.804437
240.565953	918.334902	18.675072	-0.045480	1.798279
240.403166	910.416085	18.680077	-0.045444	1.792038
240.268322	902.500072	18.685082	-0.045414	1.785781
240.222257	894.623515	18.690087	-0.045401	1.779544
239.971224	886.752437	18.695091	-0.045349	1.773264
239.997142	878.848746	18.700096	-0.045348	1.766970
239.981672	870.958544	18.705101	-0.045341	1.760659
239.885624	863.103531	18.710106	-0.045318	1.754344
239.919968	855.187804	18.715111	-0.045319	1.747973
239.715672	847.324277	18.720115	-0.045276	1.741591
239.628358	839.466416	18.725120	-0.045255	1.735205
239.341289	831.591515	18.730125	-0.045196	1.728756
239.385892	823.716489	18.735130	-0.045199	1.722325
239.458587	815.831421	18.740135	-0.045208	1.715865
239.294724	807.942936	18.745139	-0.045172	1.709348
239.145765	800.077773	18.750144	-0.045139	1.702827
239.157615	792.189126	18.755149	-0.045137	1.696282
239.307662	784.285102	18.760154	-0.045159	1.689717
239.020840	776.451760	18.765159	-0.045101	1.683128
238.781664	768.613577	18.770163	-0.045051	1.676515
238.904096	760.710211	18.775168	-0.045069	1.669870
238.862620	752.832645	18.780173	-0.045056	1.663197
238.611507	745.014282	18.785178	-0.045005	1.656520
238.601747	737.131740	18.790183	-0.044998	1.649794
238.443887	729.279774	18.795187	-0.044963	1.643046
238.480609	721.425526	18.800192	-0.044965	1.636295
238.579844	713.480534	18.805197	-0.044978	1.629446
238.376339	705.645698	18.810202	-0.044936	1.622622
238.155786	697.831136	18.815207	-0.044890	1.615784
238.030981	689.966104	18.820211	-0.044861	1.608887
238.110060	682.106070	18.825216	-0.044871	1.601992
237.991606	674.275413	18.830221	-0.044844	1.595066
237.861141	666.425563	18.835226	-0.044814	1.588091
238.036956	658.547329	18.840231	-0.044842	1.581104
237.914524	650.730451	18.845235	-0.044814	1.574098
237.767857	642.898750	18.850240	-0.044782	1.567044
237.493410	635.100419	18.855245	-0.044726	1.559969
237.577299	627.243489	18.860250	-0.044737	1.552861
237.542835	619.383181	18.865255	-0.044725	1.545700
237.321230	611.577324	18.870259	-0.044679	1.538527
237.427208	603.719290	18.875264	-0.044693	1.531322
237.269263	595.898906	18.880269	-0.044659	1.524078
237.218335	588.094362	18.885274	-0.044645	1.516831
237.104217	580.267546	18.890279	-0.044618	1.509518
236.935872	572.446810	18.895283	-0.044582	1.502166
237.113316	564.619769	18.900288	-0.044610	1.494826
236.831438	556.818513	18.905293	-0.044552	1.487403
236.757900	549.021701	18.910298	-0.044534	1.479979
236.823560	541.185792	18.915303	-0.044541	1.472503
236.566868	533.366969	18.920307	-0.044488	1.464953
236.470457	525.585895	18.925312	-0.044465	1.457427
236.478517	517.754370	18.930317	-0.044462	1.449829
236.334934	509.977560	18.935322	-0.044430	1.442220
236.192047	502.211263	18.940327	-0.044398	1.434581
236.257463	494.370089	18.945331	-0.044406	1.426861
236.023414	486.631592	18.950336	-0.044357	1.419152
235.925651	478.839698	18.955341	-0.044334	1.411370
235.799772	471.064528	18.960346	-0.044305	1.403557
235.751093	463.298740	18.965351	-0.044291	1.395722
235.569339	455.506880	18.970355	-0.044252	1.387795
235.504399	447.738575	18.975360	-0.044235	1.379865
235.420703	439.962431	18.980365	-0.044215	1.371879
235.422816	432.183306	18.985370	-0.044210	1.363857
235.354687	424.435555	18.990375	-0.044193	1.355808
235.266250	416.666459	18.995379	-0.044171	1.347686
235.157333	408.932850	19.000384	-0.044146	1.339547
235.015938	401.181987	19.005389	-0.044115	1.331335
235.110047	393.414023	19.010394	-0.044127	1.323096
235.180442	385.654992	19.015399	-0.044135	1.314811
234.927338	377.828941	19.020403	-0.044083	1.306342
234.831488	370.126966	19.025408	-0.044060	1.297981
234.704105	362.407257	19.030413	-0.044032	1.289540
234.702009	354.685546	19.035418	-0.044026	1.281065
234.627203	346.989065	19.040423	-0.044007	1.272548
234.476864	339.278531	19.045427	-0.043975	1.263944
234.528750	331.575556	19.050432	-0.043979	1.255327
234.431502	323.876200	19.055437	-0.043956	1.246627
234.108273	316.242847	19.060442	-0.043891	1.237897
234.097972	308.529970	19.065447	-0.043884	1.229074
233.830035	300.862590	19.070451	-0.043829	1.220189
233.794553	293.188608	19.075456	-0.043818	1.211278
233.732562	285.505736	19.080461	-0.043801	1.202285
233.584372	277.862617	19.085466	-0.043769	1.193253
233.588829	270.184741	19.090471	-0.043765	1.184143
233.538815	262.530995	19.095475	-0.043751	1.174979
233.534485	254.878690	19.100480	-0.043745	1.165754
233.133324	247.310085	19.105485	-0.043665	1.156476
232.966640	239.651220	19.110490	-0.043629	1.147060
232.953492	232.018391	19.115495	-0.043622	1.137631
232.761798	224.409311	19.120499	-0.043582	1.128115
232.536940	216.836470	19.125504	-0.043535	1.118556
232.276961	209.253355	19.130509	-0.043482	1.108894
231.966461	201.695467	19.135514	-0.043419	1.099169
231.444153	194.181088	19.140519	-0.043317	1.089365
230.924306	186.667187	19.145523	-0.043215	1.079473
230.622545	179.120052	19.150528	-0.043154	1.069495
230.112133	171.605223	19.155533	-0.043054	1.059418
229.767316	164.076566	19.160538	-0.042985	1.049264
229.436622	156.562232	19.165543	-0.042919	1.039034
228.962904	149.072627	19.170547	-0.042826	1.028701
228.630838	141.575876	19.175552	-0.042759	1.018288
228.270252	134.084134	19.180557	-0.042687	1.007766
227.850517	126.635107	19.185562	-0.042604	0.997180
227.546613	119.131456	19.190567	-0.042543	0.986430
226.975444	111.714849	19.195571	-0.042432	0.975620
226.766628	104.259356	19.200576	-0.042388	0.964724
226.238444	96.874325	19.205581	-0.042285	0.953726
225.706500	89.496888	19.210586	-0.042181	0.942609
225.367237	82.114420	19.215591	-0.042113	0.931403
224.557840	74.815550	19.220595	-0.041958	0.920061
223.938988	67.500382	19.225600	-0.041838	0.908605
223.257676	60.433052	19.230605	-0.041707	0.897374