Tue Mar 23 11:27:06 2021

Number of Points = 3623
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.401105	0.150203	0.000000	0.000072	0.723011

0.489729	0.137760	0.005005	0.000056	0.723018
0.225438	0.181499	0.010010	0.000105	0.723012
0.439403	0.145987	0.015014	0.000065	0.723017
0.436419	0.142493	0.020019	0.000065	0.723009
0.394393	0.152830	0.025024	0.000073	0.723015
0.430046	0.065823	0.030029	0.000066	0.722857
0.326827	0.003596	0.035034	0.000086	0.722699
0.423159	-0.008909	0.040038	0.000068	0.722708
0.308954	0.008034	0.045043	0.000089	0.722702
0.397147	-0.006680	0.050048	0.000072	0.722704
0.445867	-0.013532	0.055053	0.000063	0.722708
0.378022	-0.007426	0.060058	0.000076	0.722696
0.487585	-0.021968	0.065062	0.000055	0.722706
0.375971	-0.007156	0.070067	0.000076	0.722696
0.302219	0.008072	0.075072	0.000089	0.722700
0.222076	0.024717	0.080077	0.000104	0.722705
0.485215	-0.025713	0.085082	0.000055	0.722698
0.463027	-0.017835	0.090086	0.000059	0.722706
0.380268	-0.123831	0.095091	0.000075	0.722469
0.292551	-0.155038	0.100096	0.000091	0.722378
0.382248	-0.169186	0.105101	0.000074	0.722381
0.327787	-0.163155	0.110106	0.000084	0.722374
0.477098	-0.187439	0.115110	0.000056	0.722379
0.600495	-0.210885	0.120115	0.000033	0.722376
0.561457	-0.266009	0.125120	0.000040	0.722255
0.398078	-0.323259	0.130125	0.000071	0.722085
0.281332	-0.306574	0.135130	0.000092	0.722077
0.262658	-0.299444	0.140134	0.000096	0.722085
-0.079504	-0.241001	0.145139	0.000159	0.722080
-0.098778	-0.260814	0.150144	0.000163	0.722035
0.057003	-0.431716	0.155149	0.000134	0.721753
-0.087749	-0.409527	0.160154	0.000161	0.721747
-0.062282	-0.410059	0.165158	0.000156	0.721755
0.065891	-0.436379	0.170163	0.000132	0.721748
0.185578	-0.547534	0.175168	0.000110	0.721571
0.175362	-0.607720	0.180173	0.000112	0.721450
0.314216	-0.636616	0.185178	0.000086	0.721442
0.512883	-0.668858	0.190182	0.000049	0.721448
0.157751	-0.752811	0.195187	0.000115	0.721159
-0.271164	-0.692244	0.200192	0.000194	0.721128
-0.060760	-0.728244	0.205197	0.000155	0.721131
0.021272	-0.783001	0.210202	0.000140	0.721052
0.022195	-0.865985	0.215206	0.000140	0.720889
-0.215560	-0.826280	0.220211	0.000184	0.720884
-0.017340	-0.866576	0.225216	0.000147	0.720874
-0.116977	-1.015557	0.230221	0.000165	0.720546
-0.310549	-0.984074	0.235226	0.000201	0.720541
-0.191001	-0.999501	0.240230	0.000179	0.720552
-0.318069	-1.130448	0.245235	0.000203	0.720250
-0.121958	-1.176229	0.250240	0.000166	0.720229
-0.118280	-1.183945	0.255245	0.000165	0.720215
-0.232230	-1.323967	0.260250	0.000186	0.719899
-0.366371	-1.294507	0.265254	0.000211	0.719911
-0.451711	-1.324543	0.270259	0.000227	0.719822
-0.403052	-1.440310	0.275264	0.000218	0.719611
-0.538065	-1.413863	0.280269	0.000243	0.719616
-0.574205	-1.516953	0.285274	0.000250	0.719400
-0.396352	-1.608461	0.290278	0.000217	0.719282
-0.419828	-1.622688	0.295283	0.000221	0.719246
-0.685328	-1.717234	0.300288	0.000270	0.718966
-0.717984	-1.708738	0.305293	0.000276	0.718972
-0.779051	-1.798949	0.310298	0.000288	0.718772
-0.909586	-1.835728	0.315302	0.000312	0.718654
-1.485281	-1.749668	0.320307	0.000419	0.718622
-1.428217	-1.893030	0.325312	0.000408	0.718359
-1.091110	-1.948089	0.330317	0.000346	0.718369
-0.844971	-2.108721	0.335322	0.000300	0.718138
-0.976827	-2.139681	0.340326	0.000324	0.718031
-1.690738	-2.074249	0.345331	0.000457	0.717909
-2.393311	-2.049830	0.350336	0.000588	0.717710
-2.876274	-1.960989	0.355341	0.000677	0.717716
-3.233828	-1.997665	0.360346	0.000744	0.717518
-3.907770	-1.940521	0.365350	0.000869	0.717394
-3.556882	-2.007240	0.370355	0.000804	0.717385
-3.856428	-2.014391	0.375360	0.000860	0.717266
-4.705361	-1.949133	0.380365	0.001018	0.717096
-4.617738	-1.967626	0.385370	0.001001	0.717090
-4.578351	-1.973347	0.390374	0.000994	0.717093
-5.008483	-2.044161	0.395379	0.001074	0.716802
-5.815249	-1.921031	0.400384	0.001224	0.716761
-5.527144	-1.970378	0.405389	0.001170	0.716765
-5.841126	-1.919317	0.410394	0.001229	0.716756
-6.013505	-2.012670	0.415398	0.001261	0.716510
-6.555248	-1.944136	0.420403	0.001361	0.716455
-6.625954	-1.930843	0.425408	0.001374	0.716457
-6.283170	-1.990206	0.430413	0.001311	0.716460
-6.589297	-2.002521	0.435418	0.001367	0.716328
-7.430108	-1.944924	0.440422	0.001524	0.716145
-7.530507	-1.928745	0.445427	0.001542	0.716142
-7.946231	-1.857037	0.450432	0.001620	0.716138
-7.548144	-1.924164	0.455437	0.001546	0.716145
-7.510949	-1.972861	0.460442	0.001539	0.716062
-8.304585	-1.916500	0.465446	0.001686	0.715894
-7.948099	-1.983622	0.470451	0.001620	0.715887
-8.347349	-1.912405	0.475456	0.001694	0.715887
-8.234160	-1.929817	0.480461	0.001673	0.715893
-8.146482	-1.976033	0.485466	0.001656	0.715833
-9.087201	-1.948348	0.490470	0.001831	0.715555
-9.102272	-1.949962	0.495475	0.001834	0.715547
-9.541025	-1.872140	0.500480	0.001916	0.715547
-8.819869	-1.997877	0.505485	0.001781	0.715552
-9.138566	-1.945177	0.510490	0.001841	0.715544
-9.312217	-1.989650	0.515494	0.001873	0.715395
-9.951360	-1.956036	0.520499	0.001992	0.715236
-9.676650	-2.004934	0.525504	0.001941	0.715236
-9.933940	-1.956363	0.530509	0.001988	0.715242
-9.963717	-1.955671	0.535514	0.001994	0.715233
-9.733361	-1.993208	0.540518	0.001951	0.715240
-10.244802	-2.039771	0.545523	0.002046	0.714967
-11.085980	-1.918577	0.550528	0.002203	0.714910
-10.590765	-2.003725	0.555533	0.002110	0.714916
-10.719516	-1.984300	0.560538	0.002134	0.714910
-11.016374	-1.926834	0.565542	0.002189	0.714919
-10.559166	-2.010245	0.570547	0.002104	0.714915
-10.933065	-2.067523	0.575552	0.002174	0.714669
-11.850383	-1.929136	0.580557	0.002344	0.714620
-12.084007	-1.893387	0.585562	0.002388	0.714608
-11.298908	-2.030762	0.590566	0.002242	0.714613
-11.881137	-1.928793	0.595571	0.002350	0.714610
-12.217516	-1.869869	0.600576	0.002412	0.714608
-11.645210	-2.000858	0.605581	0.002306	0.714551
-12.805763	-1.932756	0.610586	0.002522	0.714276
-12.569016	-1.969789	0.615590	0.002478	0.714286
-12.768796	-1.935862	0.620595	0.002515	0.714283
-12.563072	-1.973616	0.625600	0.002476	0.714281
-12.536204	-1.975700	0.630605	0.002471	0.714286
-12.558709	-1.975550	0.635610	0.002475	0.714279
-12.485979	-2.066399	0.640614	0.002462	0.714124
-13.886657	-1.891242	0.645619	0.002722	0.713977
-13.816564	-1.905818	0.650624	0.002709	0.713973
-13.282726	-1.996835	0.655629	0.002610	0.713981
-13.899900	-1.890991	0.660634	0.002724	0.713973
-14.009478	-1.867633	0.665638	0.002745	0.713981
-13.811444	-1.905116	0.670643	0.002708	0.713977
-13.576986	-1.974215	0.675648	0.002664	0.713922
-14.386310	-1.960456	0.680653	0.002815	0.713663
-14.554564	-1.933554	0.685658	0.002846	0.713657
-14.385760	-1.962102	0.690662	0.002814	0.713661
-14.308639	-1.977066	0.695667	0.002800	0.713658
-14.645723	-1.918991	0.700672	0.002863	0.713655
-14.519372	-1.936445	0.705677	0.002839	0.713665
-14.469694	-1.985095	0.710682	0.002830	0.713586
-15.187799	-1.963707	0.715686	0.002963	0.713374
-15.247117	-1.956641	0.720691	0.002974	0.713367
-15.548074	-1.903078	0.725696	0.003030	0.713367
-15.420731	-1.923417	0.730701	0.003006	0.713372
-15.495755	-1.915515	0.735706	0.003020	0.713362
-15.308908	-1.946336	0.740710	0.002985	0.713367
-15.325699	-1.987091	0.745715	0.002988	0.713280
-16.672260	-1.874950	0.750720	0.003239	0.713026
-15.889921	-2.009071	0.755725	0.003093	0.713036
-16.261879	-1.948819	0.760730	0.003162	0.713024
-16.415764	-1.918317	0.765734	0.003191	0.713031
-16.367841	-1.928314	0.770739	0.003182	0.713028
-16.179604	-1.963542	0.775744	0.003147	0.713025
-16.121210	-2.006808	0.780749	0.003136	0.712960
-17.415871	-1.899694	0.785754	0.003377	0.712714
-17.236751	-1.928124	0.790758	0.003343	0.712721
-17.132745	-1.948268	0.795763	0.003324	0.712718
-17.303431	-1.920144	0.800768	0.003356	0.712714
-17.206663	-1.934217	0.805773	0.003338	0.712720
-17.283334	-1.924408	0.810778	0.003352	0.712713
-17.059867	-1.961483	0.815782	0.003310	0.712718
-17.551859	-2.019134	0.820787	0.003402	0.712429
-18.259623	-1.910763	0.825792	0.003533	0.712394
-18.161026	-1.925673	0.830797	0.003515	0.712399
-18.104281	-1.940178	0.835802	0.003504	0.712391
-18.091370	-1.938923	0.840806	0.003502	0.712398
-18.038474	-1.950471	0.845811	0.003492	0.712394
-18.307460	-1.903383	0.850816	0.003542	0.712392
-18.112237	-2.037810	0.855821	0.003505	0.712194
-18.993417	-1.931466	0.860826	0.003669	0.712093
-18.896681	-1.944872	0.865830	0.003651	0.712101
-18.893339	-1.946299	0.870835	0.003650	0.712100
-19.045154	-1.923177	0.875840	0.003679	0.712092
-18.542910	-2.007924	0.880845	0.003585	0.712101
-18.989294	-1.931229	0.885850	0.003668	0.712096
-19.517957	-1.998451	0.890854	0.003766	0.711774
-19.616141	-1.984373	0.895859	0.003785	0.711768
-19.984742	-1.920671	0.900864	0.003853	0.711764
-19.506820	-2.001794	0.905869	0.003764	0.711772
-19.822530	-1.951819	0.910874	0.003823	0.711760
-19.871494	-1.939035	0.915878	0.003832	0.711768
-19.688579	-1.985290	0.920883	0.003798	0.711741
-20.386018	-2.003698	0.925888	0.003927	0.711457
-20.755157	-1.933209	0.930893	0.003996	0.711466
-21.117252	-1.872814	0.935898	0.004063	0.711458
-20.599471	-1.963663	0.940902	0.003967	0.711461
-20.441953	-1.990875	0.945907	0.003937	0.711463
-20.788984	-1.930661	0.950912	0.004002	0.711460
-20.577559	-1.964583	0.955917	0.003963	0.711468
-21.322560	-1.994673	0.960922	0.004101	0.711143
-21.596621	-1.943274	0.965926	0.004152	0.711148
-21.578659	-1.947617	0.970931	0.004149	0.711146
-21.672201	-1.932486	0.975936	0.004166	0.711143
-21.484986	-1.961822	0.980941	0.004131	0.711151
-21.901451	-1.891738	0.985946	0.004208	0.711143
-21.677764	-1.928785	0.990950	0.004167	0.711149
-21.671051	-2.027922	0.995955	0.004165	0.710954
-22.583589	-1.905060	1.000960	0.004335	0.710875
-22.123138	-1.981244	1.005965	0.004249	0.710886
-22.154522	-1.980899	1.010970	0.004255	0.710876
-22.331430	-1.946966	1.015974	0.004288	0.710881
-22.535357	-1.910642	1.020979	0.004326	0.710881
-22.384410	-1.956031	1.025984	0.004298	0.710845
-23.100621	-1.977228	1.030989	0.004431	0.710548
-23.276355	-1.951161	1.035994	0.004464	0.710537
-23.345575	-1.936923	1.040998	0.004476	0.710541
-23.145109	-1.972337	1.046003	0.004439	0.710542
-23.499950	-1.912249	1.051008	0.004505	0.710536
-23.530805	-1.901800	1.056013	0.004511	0.710546
-23.085000	-1.989950	1.061018	0.004427	0.710529
-23.619570	-2.046172	1.066022	0.004527	0.710226
-24.394599	-1.907505	1.071027	0.004671	0.710227
-24.592755	-1.875136	1.076032	0.004708	0.710222
-23.766607	-2.018284	1.081037	0.004554	0.710230
-24.370449	-1.914491	1.086042	0.004666	0.710223
-24.695579	-1.853876	1.091046	0.004727	0.710228
-24.001182	-1.978196	1.096051	0.004597	0.710227
-24.379874	-2.056424	1.101056	0.004668	0.709936
-25.094078	-1.943540	1.106061	0.004801	0.709907
-25.438304	-1.887562	1.111066	0.004865	0.709897
-24.850295	-1.989611	1.116070	0.004755	0.709903
-25.105776	-1.944372	1.121075	0.004803	0.709902
-25.244889	-1.923614	1.126080	0.004828	0.709894
-24.686105	-2.019909	1.131085	0.004724	0.709901
-25.706618	-1.990922	1.136090	0.004914	0.709595
-25.822466	-1.967871	1.141094	0.004936	0.709600
-25.636952	-1.998790	1.146099	0.004901	0.709605
-26.126536	-1.915621	1.151104	0.004992	0.709597
-26.357138	-1.869470	1.156109	0.005035	0.709607
-25.990999	-1.938776	1.161114	0.004967	0.709599
-25.736099	-1.983619	1.166118	0.004919	0.709601
-26.624229	-1.985440	1.171123	0.005084	0.709280
-27.134879	-1.902530	1.176128	0.005179	0.709264
-26.592097	-1.994694	1.181133	0.005078	0.709274
-26.728588	-1.972722	1.186138	0.005104	0.709269
-27.248590	-1.879684	1.191142	0.005200	0.709270
-26.959883	-1.929851	1.196147	0.005146	0.709273
-26.893225	-1.944662	1.201152	0.005134	0.709267
-27.099839	-2.011518	1.206157	0.005172	0.709060
-27.997034	-1.903028	1.211162	0.005339	0.708957
-27.637101	-1.964680	1.216166	0.005272	0.708962
-27.862272	-1.924488	1.221171	0.005314	0.708963
-28.074742	-1.889521	1.226176	0.005353	0.708957
-27.551218	-1.978297	1.231181	0.005256	0.708966
-27.953609	-1.911476	1.236186	0.005331	0.708957
-28.213931	-1.926710	1.241190	0.005379	0.708833
-28.533327	-1.964207	1.246195	0.005439	0.708644
-28.284636	-2.013752	1.251200	0.005392	0.708634
-28.769127	-1.919520	1.256205	0.005482	0.708650
-28.999079	-1.882371	1.261210	0.005525	0.708643
-28.513199	-1.968923	1.266214	0.005434	0.708643
-28.594656	-1.954028	1.271219	0.005450	0.708644
-29.117160	-1.888119	1.276224	0.005547	0.708589
-29.339722	-1.963632	1.281229	0.005588	0.708359
-29.198833	-1.990071	1.286234	0.005562	0.708356
-29.715422	-1.897286	1.291238	0.005658	0.708358
-29.332143	-1.966491	1.296243	0.005586	0.708356
-29.357836	-1.964180	1.301248	0.005591	0.708352
-29.508804	-1.932031	1.306253	0.005619	0.708363
-29.715455	-1.965260	1.311258	0.005657	0.708222
-30.316181	-1.960087	1.316262	0.005769	0.708018
-29.898700	-2.033209	1.321267	0.005691	0.708021
-30.693385	-1.894445	1.326272	0.005839	0.708015
-30.220412	-1.973369	1.331277	0.005751	0.708026
-30.056286	-2.008853	1.336282	0.005721	0.708014
-30.627070	-1.906525	1.341286	0.005827	0.708015
-30.718950	-1.981570	1.346291	0.005844	0.707832
-31.611144	-1.889696	1.351296	0.006010	0.707698
-31.162928	-1.964252	1.356301	0.005926	0.707709
-31.501382	-1.908615	1.361306	0.005989	0.707699
-31.371787	-1.930435	1.366310	0.005965	0.707702
-31.065516	-1.985453	1.371315	0.005908	0.707701
-31.524599	-1.906879	1.376320	0.005993	0.707695
-31.217832	-2.002634	1.381325	0.005936	0.707613
-32.222232	-1.940125	1.386330	0.006123	0.707379
-32.012243	-1.977518	1.391334	0.006084	0.707379
-32.294186	-1.926932	1.396339	0.006136	0.707380
-32.129910	-1.959406	1.401344	0.006105	0.707374
-32.025357	-1.973110	1.406349	0.006086	0.707384
-32.581441	-1.878141	1.411354	0.006189	0.707376
-32.471518	-1.913993	1.416358	0.006169	0.707344
-32.626752	-2.014231	1.421363	0.006198	0.707087
-33.166380	-1.921103	1.426368	0.006298	0.707081
-33.290709	-1.893475	1.431373	0.006321	0.707092
-32.907717	-1.966054	1.436378	0.006250	0.707084
-33.254677	-1.904464	1.441382	0.006314	0.707083
-33.332761	-1.887682	1.446387	0.006329	0.707089
-33.227946	-1.912473	1.451392	0.006309	0.707077
-33.301248	-2.038179	1.456397	0.006323	0.706799
-34.174884	-1.905178	1.461402	0.006485	0.706753
-34.256516	-1.888853	1.466406	0.006500	0.706757
-33.634821	-1.997951	1.471411	0.006384	0.706761
-34.309413	-1.881504	1.476416	0.006510	0.706753
-34.178333	-1.901029	1.481421	0.006485	0.706761
-33.932647	-1.949098	1.486426	0.006440	0.706753
-34.394266	-1.981222	1.491430	0.006525	0.706523
-35.358774	-1.845759	1.496435	0.006705	0.706450
-34.945649	-1.923241	1.501440	0.006628	0.706442
-34.533213	-1.992058	1.506445	0.006551	0.706452
-35.022456	-1.907320	1.511450	0.006642	0.706447
-35.064945	-1.899990	1.516454	0.006650	0.706447
-34.710245	-1.959255	1.521459	0.006584	0.706455
-35.035532	-1.990510	1.526464	0.006644	0.706276
-35.999657	-1.886381	1.531469	0.006824	0.706140
-35.695951	-1.946846	1.536474	0.006767	0.706127
-35.750759	-1.936117	1.541478	0.006777	0.706129
-35.978028	-1.894380	1.546483	0.006819	0.706132
-35.861659	-1.919399	1.551488	0.006797	0.706123
-35.596992	-1.961845	1.556493	0.006748	0.706133
-35.998418	-1.948211	1.561498	0.006823	0.706017
-37.036577	-1.839432	1.566502	0.007016	0.705864
-36.334202	-1.963035	1.571507	0.006885	0.705867
-36.780023	-1.887117	1.576512	0.006968	0.705860
-36.799153	-1.880846	1.581517	0.006971	0.705866
-36.444877	-1.945861	1.586522	0.006905	0.705862
-36.596531	-1.918415	1.591526	0.006934	0.705863
-36.776197	-1.951611	1.596531	0.006967	0.705732
-37.888193	-1.860542	1.601536	0.007174	0.705517
-37.186365	-1.980484	1.606541	0.007043	0.705527
-37.660334	-1.898498	1.611546	0.007131	0.705523
-37.916207	-1.852476	1.616550	0.007179	0.705524
-37.232420	-1.972150	1.621555	0.007051	0.705528
-37.689578	-1.895371	1.626560	0.007136	0.705519
-37.512418	-1.972980	1.631565	0.007103	0.705426
-38.544923	-1.897344	1.636570	0.007296	0.705208
-38.334748	-1.934350	1.641574	0.007256	0.705210
-38.563874	-1.890730	1.646579	0.007299	0.705215
-38.378097	-1.928698	1.651584	0.007264	0.705206
-38.219306	-1.951933	1.656589	0.007235	0.705216
-38.685106	-1.870393	1.661594	0.007321	0.705213
-38.647936	-1.906172	1.666598	0.007314	0.705155
-38.809270	-2.009592	1.671603	0.007344	0.704889
-39.230693	-1.936424	1.676608	0.007423	0.704885
-39.637362	-1.860152	1.681613	0.007498	0.704893
-39.323032	-1.919559	1.686618	0.007440	0.704886
-39.448289	-1.897398	1.691622	0.007463	0.704886
-39.352126	-1.911837	1.696627	0.007445	0.704892
-39.511487	-1.897853	1.701632	0.007474	0.704863
-39.762633	-1.986755	1.706637	0.007521	0.704593
-40.040767	-1.937537	1.711642	0.007573	0.704593
-40.469186	-1.862112	1.716646	0.007652	0.704591
-40.026987	-1.939084	1.721651	0.007570	0.704595
-40.287690	-1.896032	1.726656	0.007618	0.704588
-40.246405	-1.899607	1.731661	0.007611	0.704596
-40.228291	-1.928672	1.736666	0.007607	0.704544
-40.831760	-1.964192	1.741670	0.007719	0.704256
-40.930131	-1.942874	1.746675	0.007738	0.704264
-41.377051	-1.867981	1.751680	0.007821	0.704254
-40.937801	-1.940792	1.756685	0.007739	0.704266
-41.037018	-1.926368	1.761690	0.007757	0.704259
-41.217689	-1.893438	1.766694	0.007791	0.704261
-40.936032	-1.970551	1.771699	0.007738	0.704207
-41.874690	-1.930774	1.776704	0.007913	0.703950
-42.175869	-1.874854	1.781709	0.007969	0.703954
-42.161776	-1.878073	1.786714	0.007966	0.703953
-41.963501	-1.916018	1.791718	0.007929	0.703948
-41.978626	-1.909967	1.796723	0.007932	0.703955
-42.389992	-1.839860	1.801728	0.008008	0.703949
-41.862852	-1.930508	1.806733	0.007910	0.703955
-42.002969	-2.044008	1.811738	0.007936	0.703676
-43.112043	-1.869016	1.816742	0.008143	0.703631
-42.916897	-1.900874	1.821747	0.008106	0.703637
-42.425226	-1.991931	1.826752	0.008015	0.703630
-42.842050	-1.913463	1.831757	0.008092	0.703639
-42.904302	-1.904464	1.836762	0.008104	0.703634
-42.774562	-1.953043	1.841766	0.008079	0.703583
-43.679240	-1.909806	1.846771	0.008248	0.703345
-43.872618	-1.879364	1.851776	0.008284	0.703337
-43.652365	-1.913188	1.856781	0.008243	0.703348
-43.815082	-1.888829	1.861786	0.008273	0.703339
-43.927648	-1.868735	1.866790	0.008294	0.703339
-43.385022	-1.961068	1.871795	0.008193	0.703348
-43.645255	-1.934555	1.876800	0.008241	0.703308
-44.464775	-1.936349	1.881805	0.008393	0.703010
-44.638026	-1.905706	1.886810	0.008426	0.703010
-44.521773	-1.927560	1.891814	0.008404	0.703007
-44.512791	-1.928399	1.896819	0.008402	0.703009
-45.116098	-1.824840	1.901824	0.008514	0.703001
-44.622754	-1.908972	1.906829	0.008422	0.703009
-44.237189	-1.985866	1.911834	0.008350	0.702993
-45.517593	-1.907241	1.916838	0.008589	0.702691
-45.858126	-1.844344	1.921843	0.008652	0.702695
-45.639285	-1.888116	1.926848	0.008611	0.702686
-45.336405	-1.937951	1.931853	0.008555	0.702694
-45.350281	-1.935874	1.936858	0.008557	0.702694
-45.701558	-1.875000	1.941862	0.008623	0.702690
-45.240936	-1.953379	1.946867	0.008537	0.702698
-45.816915	-1.986562	1.951872	0.008644	0.702424
-46.522436	-1.885305	1.956877	0.008775	0.702374
-46.397758	-1.907890	1.961882	0.008752	0.702374
-46.476713	-1.896642	1.966886	0.008766	0.702368
-46.267945	-1.928274	1.971891	0.008727	0.702380
-46.382608	-1.913593	1.976896	0.008749	0.702368
-46.373381	-1.911080	1.981901	0.008747	0.702377
-46.777724	-1.959246	1.986906	0.008822	0.702134
-47.167197	-1.920415	1.991910	0.008895	0.702072
-46.759505	-1.989674	1.996915	0.008819	0.702079
-47.280034	-1.899490	2.001920	0.008915	0.702074

-46.913199	-1.964948	2.011917	0.008847	0.702074
-47.385550	-1.960359	2.021914	0.008935	0.701913
-47.973558	-1.936751	2.031910	0.009044	0.701749
-47.858042	-1.956710	2.041907	0.009022	0.701751
-48.004189	-1.932451	2.051904	0.009049	0.701748
-48.168981	-1.903671	2.061901	0.009080	0.701747
-47.652662	-1.900096	2.071898	0.008983	0.701941
-47.379631	-1.918706	2.081894	0.008932	0.702002
-47.119884	-1.927143	2.091891	0.008884	0.702079
-47.421676	-1.875485	2.101888	0.008940	0.702075
-46.970800	-1.955848	2.111885	0.008856	0.702075
-47.242070	-1.907430	2.121882	0.008906	0.702076
-47.074270	-1.937790	2.131878	0.008875	0.702075
-47.087038	-1.935148	2.141875	0.008877	0.702076
-47.136139	-1.915290	2.151872	0.008886	0.702099
-46.632029	-1.872699	2.161869	0.008792	0.702367
-46.430058	-1.907296	2.171866	0.008754	0.702371
-46.284501	-1.931642	2.181862	0.008727	0.702374
-46.246914	-1.939136	2.191859	0.008720	0.702373
-45.926765	-1.886540	2.201856	0.008660	0.702595
-45.374721	-1.937384	2.211853	0.008557	0.702692
-45.430420	-1.925425	2.221850	0.008567	0.702696
-45.270858	-1.953775	2.231846	0.008537	0.702697
-45.144104	-1.888654	2.241843	0.008513	0.702874
-44.482283	-1.941369	2.251840	0.008390	0.703007
-44.716636	-1.900076	2.261837	0.008433	0.703006
-44.690821	-1.903847	2.271834	0.008428	0.703008
-43.862706	-1.925640	2.281830	0.008274	0.703262
-43.647385	-1.922211	2.291827	0.008234	0.703347
-43.808010	-1.895804	2.301824	0.008263	0.703343
-43.631876	-1.925751	2.311821	0.008230	0.703346
-43.160429	-1.864500	2.321818	0.008142	0.703640
-42.859084	-1.916999	2.331814	0.008086	0.703643
-42.892485	-1.912110	2.341811	0.008092	0.703641
-42.577399	-1.879816	2.351808	0.008033	0.703820
-41.909779	-1.933116	2.361805	0.007909	0.703953
-42.114614	-1.895616	2.371802	0.007947	0.703955
-41.821719	-1.946258	2.381798	0.007892	0.703959
-41.394442	-1.877734	2.391795	0.007812	0.704251
-41.132921	-1.917937	2.401792	0.007763	0.704264
-41.099260	-1.925080	2.411789	0.007757	0.704262
-40.866215	-1.894591	2.421786	0.007713	0.704408
-40.038213	-1.949858	2.431782	0.007559	0.704594
-40.217246	-1.918780	2.441779	0.007592	0.704593
-40.359730	-1.892162	2.451776	0.007619	0.704596
-39.518314	-1.908835	2.461773	0.007462	0.704865
-39.418883	-1.915019	2.471770	0.007443	0.704888
-39.315599	-1.931043	2.481766	0.007424	0.704894
-39.261832	-1.868607	2.491763	0.007413	0.705039
-38.395609	-1.936376	2.501760	0.007252	0.705214
-38.688942	-1.884539	2.511757	0.007306	0.705213
-38.386634	-1.938752	2.521754	0.007250	0.705213
-37.710173	-1.915296	2.531750	0.007124	0.705503
-37.583238	-1.925399	2.541747	0.007100	0.705529
-37.554010	-1.932802	2.551744	0.007094	0.705525
-37.623694	-1.856295	2.561741	0.007107	0.705654
-36.764646	-1.904210	2.571738	0.006947	0.705866
-36.639461	-1.926618	2.581734	0.006924	0.705866
-36.871531	-1.884577	2.591731	0.006967	0.705868
-35.830410	-1.944038	2.601728	0.006773	0.706122
-36.173396	-1.878226	2.611725	0.006836	0.706132
-35.817836	-1.940333	2.621722	0.006770	0.706135
-35.693814	-1.880645	2.631718	0.006746	0.706300
-35.095481	-1.912740	2.641715	0.006635	0.706450
-35.084061	-1.916233	2.651712	0.006633	0.706447
-35.189932	-1.874445	2.661709	0.006652	0.706494
-34.374928	-1.886520	2.671706	0.006500	0.706762
-34.124803	-1.931856	2.681702	0.006453	0.706760
-34.285983	-1.903383	2.691699	0.006483	0.706760
-33.496265	-1.914904	2.701696	0.006336	0.707020
-33.465691	-1.887334	2.711693	0.006330	0.707087
-33.126039	-1.948546	2.721690	0.006267	0.707086
-33.272985	-1.887507	2.731686	0.006294	0.707156
-32.396955	-1.930682	2.741683	0.006131	0.707383
-32.563977	-1.903350	2.751680	0.006162	0.707379
-32.516249	-1.912809	2.761677	0.006152	0.707377
-31.937759	-1.889873	2.771674	0.006045	0.707630
-31.617643	-1.910133	2.781670	0.005985	0.707705
-31.589528	-1.916058	2.791667	0.005979	0.707703
-31.486700	-1.876593	2.801664	0.005960	0.707819
-30.905446	-1.882747	2.811661	0.005852	0.708015
-30.596714	-1.936887	2.821658	0.005794	0.708017
-30.870406	-1.888873	2.831654	0.005845	0.708016
-29.861814	-1.907566	2.841651	0.005657	0.708339
-29.640109	-1.941322	2.851648	0.005615	0.708351
-29.551351	-1.956885	2.861645	0.005599	0.708352
-29.695677	-1.909935	2.871642	0.005625	0.708395
-28.957527	-1.917671	2.881638	0.005488	0.708643
-28.912475	-1.925172	2.891635	0.005479	0.708645
-28.981622	-1.915833	2.901632	0.005492	0.708639
-28.487246	-1.889877	2.911629	0.005400	0.708868
-27.810756	-1.962874	2.921626	0.005273	0.708964
-28.089923	-1.912913	2.931622	0.005325	0.708964
-27.965503	-1.916526	2.941619	0.005302	0.709002
-27.351387	-1.893767	2.951616	0.005187	0.709267
-27.208957	-1.918306	2.961613	0.005161	0.709269
-27.005757	-1.954298	2.971610	0.005123	0.709270
-26.597916	-1.917185	2.981606	0.005046	0.709490
-26.192799	-1.933811	2.991603	0.004971	0.709601
-26.204315	-1.931855	3.001600	0.004973	0.709601
-26.141945	-1.941542	3.011597	0.004961	0.709605
-25.418627	-1.922135	3.021594	0.004826	0.709902
-25.446509	-1.916286	3.031590	0.004831	0.709904
-25.384875	-1.929123	3.041587	0.004820	0.709900
-25.216724	-1.862254	3.051584	0.004788	0.710094
-24.720001	-1.885492	3.061581	0.004695	0.710225
-24.793364	-1.872908	3.071578	0.004709	0.710225
-24.581570	-1.852600	3.081574	0.004669	0.710341
-23.531761	-1.940681	3.091571	0.004474	0.710539
-23.651010	-1.919648	3.101568	0.004496	0.710539
-23.665567	-1.917464	3.111565	0.004498	0.710538
-23.197379	-1.857866	3.121562	0.004411	0.710824
-22.884281	-1.888193	3.131558	0.004352	0.710876
-22.882845	-1.889211	3.141555	0.004352	0.710875
-22.807947	-1.838701	3.151552	0.004338	0.711002
-22.022175	-1.910721	3.161549	0.004191	0.711138
-21.994068	-1.915198	3.171546	0.004186	0.711140
-21.999973	-1.902380	3.181542	0.004187	0.711164
-21.483928	-1.846787	3.191539	0.004090	0.711458
-21.159985	-1.905576	3.201536	0.004030	0.711457
-21.172095	-1.903711	3.211533	0.004032	0.711456
-20.990477	-1.814371	3.221530	0.003998	0.711700
-20.557742	-1.856845	3.231526	0.003917	0.711769
-20.370467	-1.892187	3.241523	0.003882	0.711765
-20.317938	-1.807466	3.251520	0.003872	0.711953
-19.509422	-1.881042	3.261517	0.003721	0.712094
-19.701536	-1.847031	3.271514	0.003757	0.712094
-19.400149	-1.861574	3.281510	0.003701	0.712172
-18.718384	-1.873403	3.291507	0.003574	0.712391
-18.862292	-1.848686	3.301504	0.003600	0.712390
-18.649303	-1.886804	3.311501	0.003560	0.712390
-18.124219	-1.840393	3.321498	0.003462	0.712669
-17.704168	-1.891030	3.331494	0.003384	0.712717
-17.715742	-1.890007	3.341491	0.003386	0.712716
-17.764414	-1.835557	3.351488	0.003395	0.712807
-16.751572	-1.905825	3.361485	0.003206	0.713027
-16.841730	-1.888486	3.371482	0.003223	0.713030
-16.906271	-1.878577	3.381478	0.003235	0.713027
-16.178801	-1.878766	3.391475	0.003099	0.713285
-16.066452	-1.859207	3.401472	0.003078	0.713364
-15.889350	-1.890891	3.411469	0.003045	0.713364
-15.975245	-1.852040	3.421466	0.003060	0.713411
-14.940157	-1.912293	3.431462	0.002868	0.713659
-15.117610	-1.880386	3.441459	0.002900	0.713659
-14.994544	-1.904487	3.451456	0.002877	0.713655
-14.942516	-1.819846	3.461453	0.002867	0.713843
-14.166758	-1.891970	3.471450	0.002723	0.713974
-14.026301	-1.918304	3.481446	0.002696	0.713972
-14.160887	-1.892776	3.491443	0.002721	0.713975
-13.491118	-1.858624	3.501440	0.002596	0.714281
-13.358356	-1.882565	3.511437	0.002572	0.714281
-13.217382	-1.906749	3.521434	0.002545	0.714283
-12.933315	-1.880229	3.531430	0.002492	0.714436
-12.281317	-1.908210	3.541427	0.002370	0.714612
-12.219507	-1.918450	3.551424	0.002359	0.714614
-12.347616	-1.896868	3.561421	0.002382	0.714611
-11.867507	-1.870906	3.571418	0.002293	0.714833
-11.478009	-1.899281	3.581414	0.002220	0.714915
-11.535040	-1.888038	3.591411	0.002231	0.714917
-11.465668	-1.862892	3.601408	0.002217	0.714992
-10.580551	-1.897463	3.611405	0.002053	0.715237
-10.261999	-1.953470	3.621402	0.001993	0.715239
-10.298334	-1.947685	3.631398	0.002000	0.715238
-10.278410	-1.874045	3.641395	0.001996	0.715391
-9.405711	-1.948414	3.651392	0.001833	0.715552
-9.543449	-1.924687	3.661389	0.001859	0.715551
-9.537516	-1.925327	3.671386	0.001857	0.715552
-8.733617	-1.948872	3.681382	0.001707	0.715790
-8.627851	-1.916715	3.691379	0.001687	0.715891
-8.426007	-1.953785	3.701376	0.001650	0.715889
-8.379281	-1.961494	3.711373	0.001641	0.715891
-8.102253	-1.913262	3.721370	0.001589	0.716085
-7.607530	-1.973113	3.731366	0.001497	0.716141
-7.902171	-1.920418	3.741363	0.001551	0.716142
-7.523773	-1.950083	3.751360	0.001481	0.716217
-7.082918	-1.910109	3.761357	0.001399	0.716452
-6.801330	-1.959290	3.771354	0.001346	0.716454
-6.902122	-1.940369	3.781350	0.001365	0.716456
-6.349865	-1.914667	3.791347	0.001261	0.716702
-6.189899	-1.914239	3.801344	0.001232	0.716760
-6.149295	-1.923461	3.811341	0.001224	0.716756
-5.920380	-1.893502	3.821338	0.001181	0.716897
-5.036006	-1.954509	3.831334	0.001016	0.717088
-5.174578	-1.929729	3.841331	0.001042	0.717089
-5.205724	-1.925344	3.851328	0.001047	0.717087
-4.510237	-1.903814	3.861325	0.000918	0.717375
-4.185597	-1.957496	3.871322	0.000857	0.717383
-4.271675	-1.940089	3.881318	0.000873	0.717388
-4.236380	-1.863805	3.891315	0.000866	0.717551
-3.218263	-1.964816	3.901312	0.000676	0.717710
-3.681386	-1.883031	3.911309	0.000762	0.717709
-3.368432	-1.932257	3.921306	0.000704	0.717723
-2.966114	-1.850588	3.931302	0.000629	0.718026
-2.825097	-1.874570	3.941299	0.000602	0.718029
-2.803577	-1.880277	3.951296	0.000598	0.718025
-2.767586	-1.735483	3.961293	0.000591	0.718324
-1.443058	-1.951104	3.971290	0.000345	0.718365
-2.123851	-1.830682	3.981286	0.000471	0.718363
-2.023430	-1.737026	3.991283	0.000452	0.718584
-1.723758	-1.756088	4.001280	0.000396	0.718652
-2.680533	-1.544169	4.011277	0.000574	0.718734
-2.194704	-1.511323	4.021274	0.000483	0.718970
-2.173100	-1.471782	4.031270	0.000479	0.719056
-1.036235	-1.560271	4.041267	0.000267	0.719281
-1.187603	-1.535156	4.051264	0.000295	0.719278
-1.173225	-1.372094	4.061261	0.000292	0.719605
-1.714955	-1.259678	4.071258	0.000393	0.719637
-1.076750	-1.235763	4.081254	0.000274	0.719908
-1.391461	-1.127122	4.091251	0.000332	0.720013
-1.347184	-1.024795	4.101248	0.000324	0.720230
-0.357099	-1.081627	4.111245	0.000139	0.720466
-1.138776	-0.884487	4.121242	0.000284	0.720580
-0.476340	-0.846630	4.131238	0.000161	0.720887
-0.510713	-0.773852	4.141235	0.000167	0.721019
-0.875936	-0.636081	4.151232	0.000235	0.721162
-0.771938	-0.512937	4.161229	0.000215	0.721441
-0.583783	-0.422450	4.171226	0.000180	0.721685
-0.249126	-0.363289	4.181222	0.000117	0.721919
-0.596926	-0.183469	4.191219	0.000182	0.722151
-0.342629	-0.108133	4.201216	0.000134	0.722388
-0.337038	0.048179	4.211213	0.000133	0.722698
-0.229115	0.171606	4.221210	0.000113	0.722978
0.000000	0.292910	4.231206	0.000070	0.723296

0.232397	0.895009	4.236211	0.000026	0.724558
0.392775	2.131617	4.241216	-0.000005	0.727031
0.970052	3.895517	4.246221	-0.000114	0.730665
1.796645	6.167458	4.251226	-0.000269	0.735347
2.462900	8.992532	4.256230	-0.000395	0.741004
3.481303	12.243452	4.261235	-0.000587	0.747546
5.284834	15.814517	4.266240	-0.000925	0.754896
6.864859	19.860985	4.271245	-0.001222	0.762984
7.403347	24.493456	4.276250	-0.001325	0.771724
8.483131	29.404556	4.281254	-0.001530	0.781047
9.552951	34.670183	4.286259	-0.001733	0.790893
10.227273	40.323452	4.291264	-0.001862	0.801179
10.959779	46.277044	4.296269	-0.002002	0.811878
11.710201	52.499034	4.301274	-0.002146	0.822905
12.480439	59.010228	4.306278	-0.002294	0.834284
12.984467	65.764261	4.311283	-0.002392	0.845838
13.527455	72.742993	4.316288	-0.002498	0.857619
14.420322	79.867764	4.321293	-0.002669	0.869579
15.001593	87.216713	4.326298	-0.002782	0.881648
15.516383	94.753606	4.331302	-0.002883	0.893834
16.263083	102.392706	4.336307	-0.003027	0.906079
16.845741	110.212824	4.341312	-0.003141	0.918395
17.435042	118.142105	4.346317	-0.003256	0.930717
18.125193	126.161042	4.351322	-0.003389	0.943038
18.963560	134.281461	4.356326	-0.003551	0.955389
19.539307	142.508911	4.361331	-0.003664	0.967672
20.012532	150.839608	4.366336	-0.003757	0.979924
22.611974	158.904743	4.371341	-0.004247	0.992174
27.638310	166.645754	4.376346	-0.005188	1.004410
28.185944	175.261163	4.381350	-0.005295	1.016632
28.681741	183.899125	4.386355	-0.005393	1.028727
29.567473	192.489693	4.391360	-0.005564	1.040708
30.536275	201.099615	4.396365	-0.005750	1.052598
31.406727	209.739649	4.401370	-0.005918	1.064371
32.340416	218.412196	4.406374	-0.006097	1.076073
33.443384	227.023399	4.411379	-0.006309	1.087607
34.181243	235.724543	4.416384	-0.006452	1.099053
35.029348	244.412307	4.421389	-0.006615	1.110389
35.443690	253.147740	4.426394	-0.006698	1.121575
36.178066	261.828692	4.431398	-0.006841	1.132651
36.710018	270.531697	4.436403	-0.006946	1.143604
37.550957	279.209567	4.441408	-0.007108	1.154487
38.413799	287.837238	4.446413	-0.007274	1.165211
38.956007	296.504020	4.451418	-0.007381	1.175818
40.288880	305.038056	4.456422	-0.007635	1.186333
41.257628	313.631656	4.461427	-0.007821	1.196751
42.318798	322.171354	4.466432	-0.008024	1.207034
43.247956	330.761347	4.471437	-0.008203	1.217262
43.921419	339.351985	4.476442	-0.008334	1.227356
44.626676	347.962327	4.481446	-0.008471	1.237395
45.174601	356.534144	4.486451	-0.008579	1.247279
45.920374	365.075387	4.491456	-0.008723	1.257088
46.792071	373.579462	4.496461	-0.008891	1.266803
47.536144	382.092795	4.501466	-0.009035	1.276431
48.912961	390.481207	4.506470	-0.009297	1.285965
49.974503	398.944408	4.511475	-0.009501	1.295453
50.341770	407.491992	4.516480	-0.009575	1.304836
51.413999	416.028110	4.521485	-0.009780	1.314267
52.127417	424.477657	4.526490	-0.009918	1.323473
52.536332	432.971979	4.531494	-0.010000	1.332609
53.151882	441.390870	4.536499	-0.010120	1.341639
53.886076	449.800913	4.541504	-0.010263	1.350620
54.514479	458.210637	4.546509	-0.010385	1.359523
55.552566	466.530288	4.551514	-0.010584	1.368345
56.834221	474.834476	4.556518	-0.010828	1.377136
57.365024	483.244660	4.561523	-0.010932	1.385851
57.606549	491.716247	4.566528	-0.010983	1.394525
58.513068	500.029345	4.571533	-0.011157	1.403097
58.887266	508.416481	4.576538	-0.011233	1.411602
59.705657	516.742498	4.581542	-0.011391	1.420068
60.248781	525.096250	4.586547	-0.011497	1.428466
60.822536	533.440987	4.591552	-0.011610	1.436811
61.184211	541.792326	4.596557	-0.011682	1.445080
61.554569	550.144380	4.601562	-0.011757	1.453304
62.170485	558.442018	4.606566	-0.011877	1.461467
63.143835	566.695480	4.611571	-0.012064	1.469599
63.639847	575.047341	4.616576	-0.012162	1.477705
64.295974	583.308441	4.621581	-0.012289	1.485705
64.874396	591.592308	4.626586	-0.012403	1.493672
65.492748	599.867384	4.631590	-0.012523	1.501594
65.769011	608.190542	4.636595	-0.012580	1.509467
66.082254	616.496716	4.641600	-0.012644	1.517288
66.601707	624.751523	4.646605	-0.012746	1.525053
67.184121	632.994809	4.651610	-0.012860	1.532777
67.922504	641.201696	4.656614	-0.013003	1.540452
68.572348	649.427797	4.661619	-0.013129	1.548093
69.098217	657.701904	4.666624	-0.013233	1.555722
69.649640	665.928254	4.671629	-0.013341	1.563274
70.149482	674.157201	4.676634	-0.013439	1.570784
70.725655	682.390926	4.681638	-0.013552	1.578274
70.974820	690.649312	4.686643	-0.013604	1.585703
71.331869	698.913637	4.691648	-0.013676	1.593118
72.175938	707.075075	4.696653	-0.013839	1.600476
72.564780	715.297753	4.701658	-0.013916	1.607790
73.148098	723.518692	4.706662	-0.014031	1.615097
73.721769	731.715098	4.711667	-0.014143	1.622348
74.115923	739.954553	4.716672	-0.014222	1.629579
74.751960	748.188188	4.721677	-0.014346	1.636806
75.062525	756.383608	4.726682	-0.014409	1.643923
75.583869	764.575215	4.731686	-0.014511	1.651036
75.804036	772.808219	4.736691	-0.014558	1.658112
76.201445	780.982285	4.741696	-0.014637	1.665131
76.657798	789.186771	4.746701	-0.014728	1.672155
76.867082	797.392842	4.751706	-0.014772	1.679118
77.377164	805.555387	4.756710	-0.014872	1.686055
77.855631	813.740703	4.761715	-0.014967	1.692978
78.036990	821.944152	4.766720	-0.015006	1.699849
78.549397	830.114397	4.771725	-0.015107	1.706708
79.295279	838.257556	4.776730	-0.015251	1.713548
80.015662	846.384392	4.781734	-0.015391	1.720343
80.186602	854.585796	4.786739	-0.015428	1.727101
80.774484	862.747132	4.791744	-0.015543	1.733854
81.219697	870.906640	4.796749	-0.015631	1.740561
81.384870	879.103353	4.801754	-0.015667	1.747237
82.082951	887.243595	4.806758	-0.015803	1.753909
82.703196	895.366945	4.811763	-0.015924	1.760531
82.870112	903.559779	4.816768	-0.015960	1.767128
83.347957	911.740947	4.821773	-0.016055	1.773730
83.639196	919.898459	4.826778	-0.016114	1.780265
84.172100	928.047010	4.831782	-0.016219	1.786799
84.603782	936.253090	4.836787	-0.016305	1.793342
85.293795	944.346230	4.841792	-0.016438	1.799803
85.858610	952.456825	4.846797	-0.016549	1.806240
86.150867	960.635981	4.851802	-0.016609	1.812674
86.572344	968.786085	4.856806	-0.016693	1.819078
86.839615	976.933114	4.861811	-0.016748	1.825439
87.413718	985.058653	4.866816	-0.016860	1.831798
87.774569	993.213502	4.871821	-0.016933	1.838132
88.260595	1001.319687	4.876826	-0.017029	1.844421
88.604032	1009.487282	4.881830	-0.017098	1.850719
88.994915	1017.635655	4.886835	-0.017176	1.856986
89.160129	1025.794420	4.891840	-0.017212	1.863214
89.664451	1033.937196	4.896845	-0.017312	1.869448
90.029830	1042.080194	4.901850	-0.017385	1.875646
90.235142	1050.219835	4.906854	-0.017429	1.881802
90.591513	1058.339037	4.911859	-0.017500	1.887940
91.166340	1066.444764	4.916864	-0.017613	1.894072
91.542033	1074.580439	4.921869	-0.017688	1.900185
91.759001	1082.705929	4.926874	-0.017734	1.906252
92.171743	1090.846081	4.931878	-0.017816	1.912333
92.606779	1098.956273	4.936883	-0.017903	1.918375
92.865555	1107.066156	4.941888	-0.017956	1.924377
93.297830	1115.188912	4.946893	-0.018042	1.930390
93.646646	1123.310857	4.951898	-0.018112	1.936374
93.841945	1131.450021	4.956902	-0.018154	1.942335
94.635431	1139.501283	4.961907	-0.018307	1.948280
94.892701	1147.695194	4.966912	-0.018361	1.954251
95.128095	1155.808500	4.971917	-0.018410	1.960143
95.325189	1163.912262	4.976922	-0.018452	1.966007
95.664488	1172.034426	4.981926	-0.018520	1.971881
95.984785	1180.138141	4.986931	-0.018585	1.977723
96.162456	1188.254064	4.991936	-0.018624	1.983541
96.641158	1196.345764	4.996941	-0.018718	1.989357
96.919259	1204.458088	5.001946	-0.018776	1.995149
97.437540	1212.533058	5.006950	-0.018877	2.000922
97.728272	1220.642665	5.011955	-0.018937	2.006680
97.779324	1228.791034	5.016960	-0.018952	2.012424
98.120427	1236.906818	5.021965	-0.019021	2.018158
98.300105	1245.005027	5.026970	-0.019060	2.023847
98.629426	1253.111112	5.031974	-0.019126	2.029541
99.190553	1261.214494	5.036979	-0.019236	2.035241
99.322033	1269.301229	5.041984	-0.019266	2.040869
99.753745	1277.388314	5.046989	-0.019352	2.046512
99.918277	1285.502326	5.051994	-0.019388	2.052132
100.289466	1293.603990	5.056998	-0.019462	2.057748
100.651855	1301.682270	5.062003	-0.019535	2.063332
101.072296	1309.750315	5.067008	-0.019619	2.068900
101.613324	1317.864545	5.072013	-0.019725	2.074496
101.960858	1325.929897	5.077018	-0.019795	2.080024
102.460413	1334.008966	5.082022	-0.019893	2.085562
102.928161	1342.112686	5.087027	-0.019986	2.091099
103.124588	1350.228969	5.092032	-0.020028	2.096603
103.440837	1358.346184	5.097037	-0.020092	2.102105
103.626921	1366.444194	5.102042	-0.020132	2.107567
103.943913	1374.618401	5.107046	-0.020196	2.113078
104.349726	1382.689236	5.112051	-0.020277	2.118514
104.871129	1390.706867	5.117056	-0.020380	2.123912
105.310225	1398.791190	5.122061	-0.020467	2.129333
105.406966	1406.915403	5.127066	-0.020490	2.134733
105.630597	1414.993471	5.132070	-0.020537	2.140102
106.034702	1423.056264	5.137075	-0.020618	2.145464
106.366523	1431.153667	5.142080	-0.020685	2.150828
106.676302	1439.261134	5.147085	-0.020748	2.156183
106.851142	1447.332620	5.152090	-0.020786	2.161489
107.052840	1455.426960	5.157094	-0.020829	2.166800
107.810174	1463.468185	5.162099	-0.020975	2.172114
108.248721	1471.537403	5.167104	-0.021062	2.177404
108.717315	1479.618236	5.172109	-0.021155	2.182691
109.367021	1487.663000	5.177114	-0.021281	2.187958
109.892270	1495.784907	5.182118	-0.021384	2.193251
110.545639	1503.838423	5.187123	-0.021511	2.198499
110.569986	1511.948199	5.192128	-0.021521	2.203713
110.996625	1520.045762	5.197133	-0.021606	2.208944
111.344737	1528.138687	5.202138	-0.021676	2.214152
111.451504	1536.233341	5.207142	-0.021701	2.219327
111.892616	1544.293791	5.212147	-0.021789	2.224498
112.388975	1552.341002	5.217152	-0.021887	2.229654
112.678902	1560.474502	5.222157	-0.021946	2.234834
112.725673	1568.566072	5.227162	-0.021960	2.239953
113.173204	1576.611496	5.232166	-0.022049	2.245068
113.517570	1584.700618	5.237171	-0.022118	2.250189
113.586323	1592.814082	5.242176	-0.022136	2.255289
113.745957	1600.912924	5.247181	-0.022172	2.260377
113.957710	1608.967675	5.252186	-0.022216	2.265430
114.193792	1617.080810	5.257190	-0.022266	2.270511
114.534673	1625.200092	5.262195	-0.022334	2.275593
115.048926	1633.205909	5.267200	-0.022436	2.280608
115.252405	1641.285355	5.272205	-0.022479	2.285630
115.246934	1649.370239	5.277210	-0.022483	2.290628
115.709768	1657.421950	5.282214	-0.022575	2.295633
116.260618	1665.458180	5.287219	-0.022683	2.300626
116.281052	1673.544384	5.292224	-0.022692	2.305594
116.622952	1681.630906	5.297229	-0.022761	2.310578
116.857430	1689.704816	5.302234	-0.022810	2.315535
117.192511	1697.752017	5.307238	-0.022877	2.320473
117.398163	1705.817016	5.312243	-0.022921	2.325400
117.969976	1713.829471	5.317248	-0.023033	2.330316
118.603523	1721.895203	5.322253	-0.023156	2.335258
119.052426	1729.930384	5.327258	-0.023245	2.340156
119.922543	1737.939981	5.332262	-0.023412	2.345063
120.145675	1746.074569	5.337267	-0.023459	2.349982
120.590438	1754.180882	5.342272	-0.023548	2.354891
120.910388	1762.247260	5.347277	-0.023613	2.359756
121.365391	1770.276335	5.352282	-0.023703	2.364600
121.688835	1778.358684	5.357286	-0.023768	2.369455
121.799275	1786.481941	5.362291	-0.023794	2.374307
121.939789	1794.553009	5.367296	-0.023826	2.379121
122.350873	1802.603573	5.372301	-0.023907	2.383934
122.333666	1810.699380	5.377306	-0.023910	2.388730
122.821334	1818.751834	5.382310	-0.024006	2.393531
123.108595	1826.823899	5.387315	-0.024065	2.398318
123.214283	1834.886284	5.392320	-0.024090	2.403075
123.653134	1842.919193	5.397325	-0.024177	2.407832
124.009888	1850.986886	5.402330	-0.024248	2.412593
124.282668	1859.057055	5.407334	-0.024305	2.417340
124.606926	1867.112948	5.412339	-0.024370	2.422073
124.882228	1875.166095	5.417344	-0.024427	2.426791
125.168830	1883.295355	5.422349	-0.024486	2.431545
125.684822	1891.358116	5.427354	-0.024587	2.436269
125.889708	1899.402539	5.432358	-0.024631	2.440949
125.986504	1907.460515	5.437363	-0.024654	2.445620
126.242997	1915.513335	5.442368	-0.024707	2.450291
126.498076	1923.595704	5.447373	-0.024760	2.454970
126.904526	1931.596797	5.452378	-0.024841	2.459605
127.076161	1939.657725	5.457382	-0.024878	2.464247
127.470874	1947.733569	5.462387	-0.024957	2.468906
127.673835	1955.803966	5.467392	-0.025000	2.473539
128.089021	1963.853895	5.472397	-0.025083	2.478167
128.452953	1971.876997	5.477402	-0.025156	2.482767
128.753992	1979.934612	5.482406	-0.025217	2.487374
129.201637	1988.007420	5.487411	-0.025306	2.491992
129.520786	1996.066859	5.492416	-0.025371	2.496583
130.017005	2004.097842	5.497421	-0.025469	2.501164
130.332576	2012.157683	5.502426	-0.025533	2.505738
130.853864	2020.208279	5.507430	-0.025635	2.510314
131.093242	2028.330576	5.512435	-0.025685	2.514902
131.237552	2036.376268	5.517440	-0.025717	2.519431
131.653486	2044.399889	5.522445	-0.025800	2.523960
131.778912	2052.485294	5.527450	-0.025829	2.528494
131.927087	2060.553316	5.532454	-0.025862	2.533011
132.132814	2068.630767	5.537459	-0.025905	2.537530
132.467314	2076.641850	5.542464	-0.025973	2.542013
132.937754	2084.672554	5.547469	-0.026066	2.546509
132.986414	2092.774512	5.552474	-0.026080	2.551006
133.190906	2100.834152	5.557478	-0.026124	2.555483
133.772738	2108.850842	5.562483	-0.026237	2.559955
133.957127	2116.890641	5.567488	-0.026277	2.564404
134.460825	2124.944076	5.572493	-0.026376	2.568874
134.501045	2133.035963	5.577498	-0.026389	2.573326
134.646389	2141.100822	5.582502	-0.026421	2.577763
135.112916	2149.138042	5.587507	-0.026514	2.582199
135.177511	2157.197054	5.592512	-0.026531	2.586612
135.226301	2165.343949	5.597517	-0.026545	2.591064
135.531495	2173.513364	5.602522	-0.026608	2.595538
135.959028	2181.449013	5.607526	-0.026693	2.599885
136.493975	2189.440373	5.612531	-0.026797	2.604263
136.538078	2197.478432	5.617536	-0.026811	2.608625
136.777810	2205.536926	5.622541	-0.026861	2.613004
137.043137	2213.565752	5.627546	-0.026916	2.617362
137.180193	2221.621930	5.632550	-0.026947	2.621718
137.336494	2229.677629	5.637555	-0.026981	2.626068
137.578940	2237.701913	5.642560	-0.027031	2.630400
137.776852	2245.770071	5.647565	-0.027074	2.634745
138.222409	2253.780507	5.652570	-0.027162	2.639069
138.326735	2261.839122	5.657574	-0.027187	2.643388
138.610641	2269.881730	5.662579	-0.027245	2.647704
138.653649	2277.974357	5.667584	-0.027258	2.652024
139.093003	2286.016670	5.672589	-0.027345	2.656335
139.262615	2294.060466	5.677594	-0.027382	2.660623
139.291631	2302.086155	5.682598	-0.027393	2.664885
139.803701	2310.139256	5.687603	-0.027494	2.669186
140.193095	2318.200430	5.692608	-0.027572	2.673476
140.409735	2326.258406	5.697613	-0.027617	2.677747
140.635297	2334.286244	5.702618	-0.027665	2.681995
140.821902	2342.321558	5.707622	-0.027705	2.686238
141.112947	2350.379123	5.712627	-0.027764	2.690493
141.325469	2358.442382	5.717632	-0.027809	2.694739
141.615801	2366.486511	5.722637	-0.027868	2.698973
141.874316	2374.519192	5.727642	-0.027922	2.703192
142.109239	2382.533312	5.732646	-0.027971	2.707394
142.557120	2390.602311	5.737651	-0.028060	2.711631
142.512157	2398.686493	5.742656	-0.028057	2.715838
143.136373	2406.648364	5.747661	-0.028178	2.720017
143.373803	2414.687407	5.752666	-0.028228	2.724205
143.691845	2422.745086	5.757670	-0.028292	2.728402
143.870389	2430.837902	5.762675	-0.028331	2.732602
143.949367	2438.889139	5.767680	-0.028351	2.736767
144.330336	2446.928598	5.772685	-0.028427	2.740939
144.750462	2454.940750	5.777690	-0.028511	2.745093
144.843192	2463.011652	5.782694	-0.028533	2.749250
145.293684	2471.120384	5.787699	-0.028623	2.753442
145.610339	2479.155069	5.792704	-0.028687	2.757582
145.786321	2487.197719	5.797709	-0.028725	2.761711
145.960482	2495.214232	5.802714	-0.028763	2.765821
146.216045	2503.225947	5.807718	-0.028816	2.769927
146.376120	2511.325770	5.812723	-0.028851	2.774065
146.430426	2519.364146	5.817728	-0.028866	2.778161
146.841464	2527.382901	5.822733	-0.028948	2.782261
147.228963	2535.394288	5.827738	-0.029026	2.786350
147.387989	2543.438518	5.832742	-0.029061	2.790436
147.717131	2551.509590	5.837747	-0.029127	2.794539
147.979123	2559.507088	5.842752	-0.029181	2.798596
148.283230	2567.567850	5.847757	-0.029243	2.802680
148.457492	2575.596540	5.852762	-0.029281	2.806736
148.672375	2583.647819	5.857766	-0.029326	2.810799
149.091658	2591.713624	5.862771	-0.029410	2.814875
149.479503	2599.715854	5.867776	-0.029487	2.818911
149.889412	2607.757825	5.872781	-0.029569	2.822963
150.247190	2615.798780	5.877786	-0.029641	2.827005
150.416602	2623.869715	5.882790	-0.029678	2.831046
150.468914	2631.968690	5.887795	-0.029693	2.835088
151.010320	2639.944873	5.892800	-0.029799	2.839091
151.393790	2647.976847	5.897805	-0.029876	2.843108
151.382689	2656.046022	5.902810	-0.029879	2.847114
151.723539	2664.065526	5.907814	-0.029948	2.851111
152.147163	2672.122504	5.912819	-0.030032	2.855124
152.163906	2680.159000	5.917824	-0.030041	2.859099
152.425711	2688.183684	5.922829	-0.030095	2.863077
152.634422	2696.228147	5.927834	-0.030139	2.867056
153.121298	2704.256039	5.932838	-0.030235	2.871036
153.303536	2712.352788	5.937843	-0.030274	2.875028
153.402624	2720.361995	5.942848	-0.030298	2.878966
153.858979	2728.378887	5.947853	-0.030388	2.882923
153.973117	2736.437313	5.952858	-0.030415	2.886876
154.285596	2744.463835	5.957862	-0.030478	2.890818
154.595948	2752.551623	5.962867	-0.030541	2.894785
154.621025	2760.568746	5.967872	-0.030551	2.898696
154.927340	2768.612601	5.972877	-0.030614	2.902631
155.384261	2776.628525	5.977882	-0.030704	2.906554
155.676052	2784.660132	5.982886	-0.030764	2.910471
156.217035	2792.790740	5.987891	-0.030870	2.914444
156.423312	2800.774537	5.992896	-0.030914	2.918322
156.595804	2808.822483	5.997901	-0.030951	2.922225
156.735438	2816.853178	6.002906	-0.030982	2.926112
156.869844	2824.873188	6.007910	-0.031013	2.929989
157.645172	2832.891454	6.012915	-0.031162	2.933893
157.633846	2840.938454	6.017920	-0.031166	2.937764
157.804790	2848.979629	6.022925	-0.031203	2.941637
158.090843	2857.000209	6.027930	-0.031261	2.945501
158.350095	2865.035671	6.032934	-0.031315	2.949366
158.672536	2873.108968	6.037939	-0.031380	2.953247
158.754606	2881.152841	6.042944	-0.031401	2.957097
159.057572	2889.176399	6.047949	-0.031463	2.960943
159.332671	2897.182740	6.052954	-0.031519	2.964774
159.419724	2905.266232	6.057958	-0.031541	2.968627
159.929803	2913.296848	6.062963	-0.031641	2.972472
159.949471	2921.358684	6.067968	-0.031650	2.976302
160.170458	2929.353581	6.072973	-0.031697	2.980105
160.392549	2937.358699	6.077978	-0.031743	2.983908
160.726604	2945.407225	6.082982	-0.031811	2.987733
160.843941	2953.502333	6.087987	-0.031838	2.991564
160.906004	2961.577296	6.092992	-0.031855	2.995377
161.156416	2969.567227	6.097997	-0.031907	2.999155
161.405745	2977.578768	6.103002	-0.031959	3.002938
161.695967	2985.575669	6.108006	-0.032018	3.006712
162.081223	2993.602786	6.113011	-0.032095	3.010499
162.352976	3001.663388	6.118016	-0.032151	3.014292
162.700975	3009.713682	6.123021	-0.032221	3.018079
162.950897	3017.746396	6.128026	-0.032273	3.021848
163.310460	3025.737782	6.133030	-0.032345	3.025599
163.564466	3033.801094	6.138035	-0.032398	3.029373
163.867317	3041.854136	6.143040	-0.032460	3.033140
164.123417	3049.918149	6.148045	-0.032513	3.036905
164.154343	3057.955671	6.153050	-0.032524	3.040643
164.357702	3065.949726	6.158054	-0.032567	3.044363
164.631053	3073.999049	6.163059	-0.032623	3.048109
164.911236	3082.034787	6.168064	-0.032681	3.051843
165.106569	3090.110125	6.173069	-0.032722	3.055587
165.381862	3098.106177	6.178074	-0.032779	3.059294
165.834400	3106.098103	6.183078	-0.032868	3.063003
166.153740	3114.162970	6.188083	-0.032933	3.066734
166.348144	3122.196876	6.193088	-0.032975	3.070441
166.703493	3130.333048	6.198093	-0.033046	3.074198
167.039745	3138.337729	6.203098	-0.033114	3.077888
167.095682	3146.340253	6.208102	-0.033130	3.081561
167.591760	3154.314233	6.213107	-0.033228	3.085236
167.880628	3162.346095	6.218112	-0.033287	3.088924
167.898126	3170.414212	6.223117	-0.033295	3.092611
168.345183	3178.433969	6.228122	-0.033384	3.096292
168.469545	3186.460755	6.233126	-0.033412	3.099956
168.718586	3194.520371	6.238131	-0.033464	3.103637
168.850469	3202.538823	6.243136	-0.033494	3.107290
169.210851	3210.569567	6.248141	-0.033566	3.110954
169.607336	3218.599510	6.253146	-0.033646	3.114614
169.944286	3226.618106	6.258150	-0.033714	3.118263
170.198458	3234.682733	6.263155	-0.033766	3.121925
170.341949	3242.666971	6.268160	-0.033798	3.125541
170.454933	3250.736861	6.273165	-0.033825	3.129190
170.747865	3258.768125	6.278170	-0.033885	3.132825
170.891352	3266.801994	6.283174	-0.033917	3.136450
171.340047	3274.829331	6.288179	-0.034005	3.140082
171.543961	3282.833050	6.293184	-0.034049	3.143688
171.959652	3290.881148	6.298189	-0.034131	3.147320
172.064653	3298.937553	6.303194	-0.034156	3.150937
172.242229	3307.003921	6.308198	-0.034195	3.154557
172.769858	3315.016502	6.313203	-0.034298	3.158165
173.060042	3323.013180	6.318208	-0.034358	3.161751
173.063406	3331.043894	6.323213	-0.034364	3.165335
173.276906	3339.078251	6.328218	-0.034409	3.168927
173.467026	3347.134600	6.333222	-0.034449	3.172523
173.697750	3355.192095	6.338227	-0.034498	3.176117
173.815030	3363.176165	6.343232	-0.034525	3.179669
173.958367	3371.223053	6.348237	-0.034557	3.183247
174.268054	3379.246350	6.353242	-0.034620	3.186817
174.504761	3387.282201	6.358246	-0.034669	3.190385
174.962748	3395.334476	6.363251	-0.034760	3.193966
175.217747	3403.353691	6.368256	-0.034813	3.197520
175.360683	3411.395357	6.373261	-0.034845	3.201075
175.596470	3419.368573	6.378266	-0.034894	3.204600
175.914383	3427.418175	6.383270	-0.034958	3.208157
176.423446	3435.484539	6.388275	-0.035059	3.211727
176.465697	3443.501397	6.393280	-0.035072	3.215251
176.806377	3451.543368	6.398285	-0.035140	3.218794
177.094678	3459.576452	6.403290	-0.035199	3.222328
177.161651	3467.584851	6.408294	-0.035217	3.225837
177.422034	3475.637641	6.413299	-0.035271	3.229371
177.784020	3483.681410	6.418304	-0.035344	3.232900
178.229533	3491.730741	6.423309	-0.035432	3.236431
178.376956	3499.729139	6.428314	-0.035465	3.239924
178.547681	3507.716893	6.433318	-0.035502	3.243410
178.826457	3515.769479	6.438323	-0.035559	3.246925
178.874001	3523.804655	6.443328	-0.035573	3.250418
179.270050	3531.843306	6.448333	-0.035652	3.253924
179.783751	3539.857056	6.453338	-0.035753	3.257419
179.929793	3547.849644	6.458342	-0.035786	3.260887
180.294943	3555.880029	6.463347	-0.035859	3.264376
180.527632	3563.944915	6.468352	-0.035908	3.267871
180.663353	3571.996931	6.473357	-0.035938	3.271353
180.823219	3580.025730	6.478362	-0.035974	3.274823
181.191929	3588.019695	6.483366	-0.036048	3.278281
181.439836	3596.078128	6.488371	-0.036099	3.281759
181.333156	3604.055659	6.493376	-0.036084	3.285185
181.773659	3612.106766	6.498381	-0.036172	3.288660
182.062693	3620.169922	6.503386	-0.036231	3.292130
182.250998	3628.187286	6.508390	-0.036271	3.295573
182.416243	3636.239987	6.513395	-0.036307	3.299027
182.505649	3644.238546	6.518400	-0.036329	3.302451
182.818826	3652.252734	6.523405	-0.036393	3.305887
183.013883	3660.290957	6.528410	-0.036435	3.309325
183.168875	3668.349958	6.533414	-0.036469	3.312767
183.722123	3676.400801	6.538419	-0.036577	3.316216
183.869213	3684.374730	6.543424	-0.036610	3.319614
184.068436	3692.397919	6.548429	-0.036652	3.323032
184.275685	3700.429507	6.553434	-0.036696	3.326449
184.709984	3708.396684	6.558438	-0.036782	3.329844
184.951691	3716.493613	6.563443	-0.036833	3.333284
185.020180	3724.540229	6.568448	-0.036851	3.336692
185.277235	3732.548532	6.573453	-0.036904	3.340088
185.282309	3740.588315	6.578458	-0.036910	3.343484
185.309210	3748.623302	6.583462	-0.036921	3.346875
185.708596	3756.666358	6.588467	-0.037000	3.350280
185.786030	3764.706047	6.593472	-0.037020	3.353668
185.959557	3772.742732	6.598477	-0.037058	3.357055
186.253396	3780.735748	6.603482	-0.037118	3.360425
186.301683	3788.753348	6.608486	-0.037132	3.363793
186.463147	3796.789521	6.613491	-0.037167	3.367169
186.631588	3804.823562	6.618496	-0.037204	3.370541
187.228391	3812.844492	6.623501	-0.037321	3.373919
187.398559	3820.894007	6.628506	-0.037358	3.377291
187.598961	3828.883309	6.633510	-0.037400	3.380635
187.886323	3836.892795	6.638515	-0.037459	3.383988
187.842905	3844.958267	6.643520	-0.037456	3.387349
187.975092	3853.020832	6.648525	-0.037486	3.390711
188.454018	3861.127168	6.653530	-0.037581	3.394100
188.708854	3869.088359	6.658534	-0.037634	3.397418
188.603500	3877.117395	6.663539	-0.037619	3.400748
188.972214	3885.091727	6.668544	-0.037693	3.404069
189.241384	3893.092788	6.673549	-0.037749	3.407394
189.318219	3901.161382	6.678554	-0.037768	3.410737
189.499647	3909.174977	6.683558	-0.037807	3.414057
190.008556	3917.206693	6.688563	-0.037907	3.417393
190.229506	3925.197384	6.693568	-0.037954	3.420699
190.208074	3933.227787	6.698573	-0.037955	3.424010
190.533424	3941.244592	6.703578	-0.038021	3.427324
190.808878	3949.269569	6.708582	-0.038078	3.430636
190.979529	3957.330668	6.713587	-0.038115	3.433956
191.215344	3965.355617	6.718592	-0.038164	3.437260
191.580041	3973.328559	6.723597	-0.038237	3.440544
191.810696	3981.375677	6.728602	-0.038286	3.443851
192.012727	3989.404723	6.733606	-0.038329	3.447146
192.324113	3997.444264	6.738611	-0.038392	3.450446
192.512347	4005.485428	6.743616	-0.038432	3.453740
192.706719	4013.532346	6.748621	-0.038474	3.457033
192.909762	4021.534290	6.753626	-0.038517	3.460304
193.274339	4029.552583	6.758630	-0.038590	3.463584
193.699407	4037.619900	6.763635	-0.038675	3.466883
193.801550	4045.624568	6.768640	-0.038699	3.470143
194.110581	4053.682046	6.773645	-0.038762	3.473428
194.389077	4061.739697	6.778650	-0.038819	3.476709
194.556230	4069.677523	6.783654	-0.038855	3.479935
194.929786	4077.701497	6.788659	-0.038930	3.483199
195.189266	4085.724308	6.793664	-0.038984	3.486456
195.338462	4093.736278	6.798669	-0.039017	3.489702
195.333082	4101.832658	6.803674	-0.039021	3.492974
195.576734	4109.819181	6.808678	-0.039072	3.496207
195.945154	4117.832261	6.813683	-0.039146	3.499451
195.951593	4125.867568	6.818688	-0.039152	3.502689
196.285857	4133.852641	6.823693	-0.039220	3.505915
196.545918	4141.907576	6.828698	-0.039274	3.509163
196.495620	4149.974317	6.833702	-0.039270	3.512404
196.766277	4158.014771	6.838707	-0.039325	3.515641
197.057736	4165.998905	6.843712	-0.039385	3.518853
197.294662	4173.998495	6.848717	-0.039434	3.522066
197.621071	4182.015921	6.853722	-0.039501	3.525287
197.722596	4190.047597	6.858726	-0.039525	3.528503
197.970041	4198.121816	6.863731	-0.039576	3.531738
198.055677	4206.131190	6.868736	-0.039597	3.534939
198.443506	4214.175430	6.873741	-0.039675	3.538160
198.679203	4222.207946	6.878746	-0.039724	3.541369
198.574181	4230.205698	6.883750	-0.039710	3.544550
198.980376	4238.249689	6.888755	-0.039791	3.547763
199.233403	4246.259828	6.893760	-0.039843	3.550955
199.328482	4254.415544	6.898765	-0.039866	3.554197
199.545045	4262.398236	6.903770	-0.039912	3.557370
199.732979	4270.338261	6.908774	-0.039952	3.560524
200.146507	4278.360415	6.913779	-0.040035	3.563713
200.051101	4286.410447	6.918784	-0.040022	3.566896
200.363077	4294.385901	6.923789	-0.040086	3.570058
200.614336	4302.452044	6.928794	-0.040138	3.573252
200.717280	4310.475304	6.933798	-0.040162	3.576421
200.872207	4318.485355	6.938803	-0.040196	3.579584
201.207761	4326.491175	6.943808	-0.040264	3.582748
201.402702	4334.517482	6.948813	-0.040306	3.585912
201.769493	4342.528370	6.953818	-0.040379	3.589073
201.924417	4350.539335	6.958822	-0.040414	3.592225
202.393856	4358.597918	6.963827	-0.040506	3.595402
202.399945	4366.605904	6.968832	-0.040513	3.598543
202.600465	4374.621502	6.973837	-0.040555	3.601689
203.102739	4382.610178	6.978842	-0.040654	3.604831
203.235436	4390.632032	6.983846	-0.040684	3.607973
203.649181	4398.693194	6.988851	-0.040767	3.611135
203.990130	4406.721913	6.993856	-0.040835	3.614279
204.060793	4414.757409	6.998861	-0.040854	3.617416
204.298905	4422.769854	7.003866	-0.040904	3.620546
204.454558	4430.775013	7.008870	-0.040938	3.623668
204.697663	4438.831677	7.013875	-0.040988	3.626810
204.867972	4446.825749	7.018880	-0.041025	3.629922
205.239932	4454.894120	7.023885	-0.041100	3.633066
205.505028	4462.970541	7.028890	-0.041155	3.636208
205.557957	4470.915534	7.033894	-0.041170	3.639290
205.816259	4478.960519	7.038899	-0.041223	3.642414
206.167435	4486.960237	7.043904	-0.041294	3.645520
206.366867	4494.990948	7.048909	-0.041337	3.648632
206.611241	4503.048207	7.053914	-0.041387	3.651752
206.737967	4511.054065	7.058918	-0.041416	3.654846
206.933743	4519.118809	7.063923	-0.041458	3.657963
207.015163	4527.127685	7.068928	-0.041479	3.661052
207.200601	4535.121831	7.073933	-0.041518	3.664136
207.735736	4543.164464	7.078938	-0.041623	3.667244
207.856364	4551.153936	7.083942	-0.041651	3.670319
208.065327	4559.215873	7.088947	-0.041695	3.673421
208.429114	4567.235457	7.093952	-0.041768	3.676509
208.524015	4575.202263	7.098957	-0.041791	3.679566
208.697380	4583.262707	7.103962	-0.041829	3.682659
208.964528	4591.231699	7.108966	-0.041884	3.685717
209.359018	4599.288949	7.113971	-0.041963	3.688809
209.471683	4607.364100	7.118976	-0.041989	3.691898
209.560835	4615.364173	7.123981	-0.042011	3.694956
209.967779	4623.396237	7.128986	-0.042092	3.698031
210.041715	4631.383702	7.133990	-0.042111	3.701078
210.198240	4639.412665	7.138995	-0.042146	3.704140
210.437061	4647.447186	7.144000	-0.042195	3.707204
210.624537	4655.450680	7.149005	-0.042236	3.710252
210.742908	4663.579492	7.154010	-0.042263	3.713344
210.921699	4671.609303	7.159014	-0.042302	3.716397
211.210043	4679.566428	7.164019	-0.042361	3.719423
211.404529	4687.565744	7.169024	-0.042402	3.722459
211.473819	4695.540791	7.174029	-0.042420	3.725481
211.877755	4703.586407	7.179034	-0.042501	3.728536
212.148174	4711.605014	7.184038	-0.042557	3.731574
212.189503	4719.634617	7.189043	-0.042570	3.734609
212.285683	4727.681440	7.194048	-0.042593	3.737649
212.486227	4735.678729	7.199053	-0.042636	3.740670
213.011737	4743.698188	7.204058	-0.042739	3.743704
212.990840	4751.721466	7.209062	-0.042740	3.746725
213.446330	4759.753589	7.214067	-0.042830	3.749758
213.475909	4767.794329	7.219072	-0.042841	3.752781
213.380973	4775.855802	7.224077	-0.042829	3.755808
213.835188	4783.870468	7.229082	-0.042919	3.758826
213.896827	4791.853058	7.234086	-0.042935	3.761822
214.063173	4799.853238	7.239091	-0.042972	3.764823
214.350129	4807.885170	7.244096	-0.043030	3.767837
214.509095	4815.882912	7.249101	-0.043065	3.770833
214.718534	4823.988510	7.254106	-0.043110	3.773868
214.780108	4831.974912	7.259110	-0.043127	3.776853
215.081738	4839.998623	7.264115	-0.043188	3.779854
215.185513	4848.031328	7.269120	-0.043213	3.782852
215.444014	4855.996813	7.274125	-0.043266	3.785826
215.836747	4864.047201	7.279130	-0.043345	3.788833
216.113076	4872.061442	7.284134	-0.043401	3.791820
216.328829	4880.159596	7.289139	-0.043447	3.794835
216.722021	4888.131229	7.294144	-0.043525	3.797805
216.921039	4896.123046	7.299149	-0.043568	3.800776
216.955583	4904.137437	7.304154	-0.043579	3.803749
217.157878	4912.151003	7.309158	-0.043622	3.806723
217.537506	4920.158239	7.314163	-0.043698	3.809696
217.515503	4928.242955	7.319168	-0.043700	3.812687
217.769063	4936.235546	7.324173	-0.043752	3.815647
218.085901	4944.270609	7.329178	-0.043817	3.818622
218.123134	4952.265275	7.334182	-0.043829	3.821574
218.328102	4960.271093	7.339187	-0.043872	3.824531
218.519846	4968.312759	7.344192	-0.043913	3.827499
218.984688	4976.314953	7.349197	-0.044005	3.830455
218.938311	4984.380039	7.354202	-0.044002	3.833422
219.102275	4992.387016	7.359206	-0.044038	3.836370
219.450329	5000.380692	7.364211	-0.044108	3.839314
219.761591	5008.414168	7.369216	-0.044171	3.842269
219.863182	5016.389720	7.374221	-0.044195	3.845197
220.016349	5024.472526	7.379226	-0.044229	3.848163
220.192318	5032.470013	7.384230	-0.044267	3.851096
220.395700	5040.517418	7.389235	-0.044310	3.854045
220.478420	5048.607509	7.394240	-0.044331	3.857005
220.784753	5056.544789	7.399245	-0.044393	3.859912
221.134248	5064.583377	7.404250	-0.044464	3.862854
221.171340	5072.580790	7.409254	-0.044476	3.865773
221.386649	5080.633866	7.414259	-0.044522	3.868713
221.693853	5088.689140	7.419264	-0.044584	3.871654
221.716509	5096.933912	7.424269	-0.044594	3.874656
221.987614	5104.868894	7.429274	-0.044650	3.877547
222.277680	5112.760809	7.434278	-0.044709	3.880421
222.554808	5120.778907	7.439283	-0.044766	3.883339
222.660012	5128.769970	7.444288	-0.044791	3.886241
222.812691	5136.774924	7.449293	-0.044824	3.889147
223.118376	5144.822829	7.454298	-0.044887	3.892069
223.287847	5152.835651	7.459302	-0.044923	3.894974
223.525887	5160.853600	7.464307	-0.044973	3.897880
223.656071	5168.871072	7.469312	-0.045003	3.900781
223.758312	5176.855373	7.474317	-0.045027	3.903668
224.076088	5184.891778	7.479322	-0.045091	3.906575
224.221834	5192.901467	7.484326	-0.045124	3.909467
224.494643	5200.955802	7.489331	-0.045180	3.912375
224.554171	5209.010495	7.494336	-0.045196	3.915278
224.724275	5216.977164	7.499341	-0.045233	3.918149
225.130901	5224.995277	7.504346	-0.045314	3.921040
225.266857	5232.972968	7.509350	-0.045345	3.923910
225.451924	5241.035878	7.514355	-0.045385	3.926809
225.917239	5248.992696	7.519360	-0.045477	3.929673
226.087664	5257.024855	7.524365	-0.045514	3.932556
226.395361	5265.104218	7.529370	-0.045576	3.935457
226.535237	5273.121967	7.534374	-0.045608	3.938330
226.780685	5281.111721	7.539379	-0.045659	3.941193
226.854183	5289.127050	7.544384	-0.045678	3.944061
226.899372	5297.139123	7.549389	-0.045692	3.946924
227.230626	5305.164341	7.554394	-0.045759	3.949795
227.252349	5313.204175	7.559398	-0.045768	3.952664
227.438335	5321.281490	7.564403	-0.045808	3.955547
227.699826	5329.261276	7.569408	-0.045862	3.958394
227.980211	5337.246914	7.574413	-0.045919	3.961242
228.126011	5345.256148	7.579418	-0.045952	3.964093
228.163729	5353.277144	7.584422	-0.045964	3.966945
228.596041	5361.261851	7.589427	-0.046050	3.969789
228.819597	5369.353643	7.594432	-0.046097	3.972665
228.905859	5377.345030	7.599437	-0.046118	3.975501
229.075588	5385.381510	7.604442	-0.046155	3.978352
229.246499	5393.379694	7.609446	-0.046192	3.981188
229.463121	5401.386875	7.614451	-0.046238	3.984025
229.834144	5409.427305	7.619456	-0.046312	3.986875
230.021970	5417.443038	7.624461	-0.046353	3.989711
230.130520	5425.488461	7.629466	-0.046378	3.992554
230.194209	5433.544335	7.634470	-0.046396	3.995399
230.582414	5441.556112	7.639475	-0.046473	3.998230
230.637896	5449.568994	7.644480	-0.046489	4.001055
230.858860	5457.555436	7.649485	-0.046535	4.003871
231.057825	5465.607139	7.654490	-0.046578	4.006708
231.360230	5473.604167	7.659494	-0.046639	4.009525
231.467720	5481.660766	7.664499	-0.046665	4.012358
231.549777	5489.708207	7.669504	-0.046685	4.015185
231.841547	5497.682005	7.674509	-0.046745	4.017988
231.966427	5505.717653	7.679514	-0.046773	4.020807
232.172512	5513.703839	7.684518	-0.046817	4.023609
232.149973	5521.747333	7.689523	-0.046818	4.026425
232.295064	5529.794710	7.694528	-0.046851	4.029244
232.531456	5537.789461	7.699533	-0.046900	4.032043
232.982033	5545.945333	7.704538	-0.046989	4.034899
233.135431	5553.864703	7.709542	-0.047023	4.037667
233.262707	5561.844363	7.714547	-0.047052	4.040453
233.539250	5569.835057	7.719552	-0.047109	4.043244
233.702454	5577.804696	7.724557	-0.047144	4.046023
233.694330	5585.883774	7.729562	-0.047148	4.048837
233.857348	5593.913927	7.734566	-0.047184	4.051633
234.051092	5601.952949	7.739571	-0.047225	4.054432
234.321185	5609.945098	7.744576	-0.047281	4.057213
234.422980	5617.914544	7.749581	-0.047305	4.059982
234.810174	5625.990558	7.754586	-0.047383	4.062790
234.939578	5633.953808	7.759590	-0.047412	4.065553
235.281732	5642.008737	7.764595	-0.047481	4.068349
235.430236	5650.046329	7.769600	-0.047514	4.071134
235.683712	5658.055598	7.774605	-0.047567	4.073909
235.757295	5666.128938	7.779610	-0.047586	4.076702
235.843867	5674.069083	7.784614	-0.047607	4.079448
236.198389	5682.108263	7.789619	-0.047678	4.082229
236.339294	5690.101567	7.794624	-0.047710	4.084989
236.428103	5698.128597	7.799629	-0.047732	4.087759
236.896577	5706.148485	7.804634	-0.047824	4.090529
236.982826	5714.188479	7.809638	-0.047846	4.093299
237.109824	5722.217910	7.814643	-0.047875	4.096064
237.292521	5730.224409	7.819648	-0.047914	4.098820
237.458853	5738.243351	7.824653	-0.047950	4.101579
237.788529	5746.210796	7.829658	-0.048017	4.104319
237.770526	5754.282966	7.834662	-0.048019	4.107090
238.101573	5762.270397	7.839667	-0.048086	4.109834
238.394485	5770.352169	7.844672	-0.048146	4.112608
238.430763	5778.320283	7.849677	-0.048158	4.115337
238.790707	5786.419796	7.854682	-0.048230	4.118115
239.025499	5794.415306	7.859686	-0.048279	4.120853
239.241288	5802.413262	7.864691	-0.048325	4.123589
239.489149	5810.417319	7.869696	-0.048376	4.126327
239.699690	5818.387868	7.874701	-0.048421	4.129050
239.997274	5826.452261	7.879706	-0.048481	4.131805
239.922338	5834.495778	7.884710	-0.048473	4.134547
239.944078	5842.553171	7.889715	-0.048482	4.137292
240.185331	5850.506547	7.894720	-0.048532	4.140003
240.379066	5858.525614	7.899725	-0.048574	4.142734
240.624357	5866.552895	7.904730	-0.048625	4.145466
240.725389	5874.583121	7.909734	-0.048649	4.148196
240.909021	5882.591990	7.914739	-0.048688	4.150918
241.100129	5890.665768	7.919744	-0.048729	4.153660
241.374274	5898.667608	7.924749	-0.048786	4.156377
241.605623	5906.651342	7.929754	-0.048834	4.159085
241.486886	5914.709082	7.934758	-0.048817	4.161813
241.956152	5922.697457	7.939763	-0.048910	4.164522
242.200481	5930.722560	7.944768	-0.048961	4.167239
242.216955	5938.697551	7.949773	-0.048969	4.169934
242.598193	5946.761219	7.954778	-0.049045	4.172662
242.625852	5954.766690	7.959782	-0.049056	4.175365
242.994384	5962.777652	7.964787	-0.049130	4.178072
243.068023	5970.805127	7.969792	-0.049149	4.180779
243.313751	5978.782390	7.974797	-0.049200	4.183469
243.525817	5986.818818	7.979802	-0.049245	4.186177
243.564516	5994.843637	7.984806	-0.049257	4.188878
243.861252	6002.865718	7.989811	-0.049318	4.191578
244.126594	6010.995366	7.994816	-0.049373	4.194313
244.121815	6018.979614	7.999821	-0.049377	4.196994
244.434794	6026.904480	8.004826	-0.049441	4.199657
244.784680	6034.935834	8.009830	-0.049511	4.202354
245.005048	6042.898087	8.014835	-0.049557	4.205025
245.041338	6051.005211	8.019840	-0.049569	4.207740
245.285198	6058.954752	8.024845	-0.049620	4.210404
245.718566	6067.012198	8.029850	-0.049706	4.213103
245.697697	6074.997554	8.034854	-0.049708	4.215773
245.849482	6083.003562	8.039859	-0.049741	4.218449
246.237267	6091.060355	8.044864	-0.049819	4.221142
246.207440	6098.978017	8.049869	-0.049818	4.223784
246.247155	6107.086919	8.054874	-0.049831	4.226488
246.601670	6115.053517	8.059878	-0.049903	4.229146
246.776093	6123.133445	8.064883	-0.049940	4.231839
246.873262	6131.189766	8.069888	-0.049964	4.234521
246.938183	6139.177949	8.074893	-0.049981	4.237178
247.125840	6147.189449	8.079898	-0.050021	4.239843
247.197270	6155.174429	8.084902	-0.050040	4.242496
247.501214	6163.150678	8.089907	-0.050102	4.245147
247.758141	6171.199190	8.094912	-0.050155	4.247819
247.918980	6179.193258	8.099917	-0.050190	4.250471
248.448398	6187.263775	8.104922	-0.050294	4.253150
248.578011	6195.324555	8.109926	-0.050324	4.255820
248.634855	6203.314955	8.114931	-0.050340	4.258464
248.918388	6211.359307	8.119936	-0.050398	4.261127
249.211935	6219.304618	8.124941	-0.050458	4.263756
249.463539	6227.369480	8.129946	-0.050510	4.266422
249.534927	6235.366434	8.134950	-0.050528	4.269062
249.592782	6243.412260	8.139955	-0.050545	4.271716
249.864850	6251.454048	8.144960	-0.050601	4.274370
249.901831	6259.505758	8.149965	-0.050613	4.277023
250.048355	6267.480159	8.154970	-0.050645	4.279650
250.125911	6275.503896	8.159974	-0.050665	4.282291
250.523437	6283.434764	8.164979	-0.050744	4.284902
250.635499	6291.532292	8.169984	-0.050771	4.287564
250.591671	6299.520665	8.174989	-0.050768	4.290187
250.798667	6307.575624	8.179994	-0.050812	4.292833
250.943714	6315.598044	8.184998	-0.050844	4.295466
251.161357	6323.590448	8.190003	-0.050890	4.298088
251.399469	6331.573067	8.195008	-0.050939	4.300705
251.287964	6339.630518	8.200013	-0.050924	4.303342
251.727760	6347.632853	8.205018	-0.051011	4.305964
251.762134	6355.643491	8.210022	-0.051023	4.308584
252.084422	6363.663225	8.215027	-0.051088	4.311208
252.156791	6371.724009	8.220032	-0.051107	4.313841
252.455529	6379.713129	8.225037	-0.051168	4.316451
252.697254	6387.666308	8.230042	-0.051218	4.319047
252.650111	6395.755966	8.235046	-0.051215	4.321684
252.788514	6403.723028	8.240051	-0.051246	4.324281
253.023100	6411.769669	8.245056	-0.051295	4.326903
253.069671	6419.776217	8.250061	-0.051309	4.329509
253.307510	6427.806768	8.255066	-0.051359	4.332123
253.397854	6435.806813	8.260070	-0.051381	4.334723
253.609767	6443.879462	8.265075	-0.051425	4.337347
253.882838	6451.836601	8.270080	-0.051482	4.339932
254.022271	6459.831055	8.275085	-0.051513	4.342527
254.332110	6467.889657	8.280090	-0.051576	4.345142
254.521664	6475.883275	8.285094	-0.051616	4.347733
254.567495	6483.898939	8.290099	-0.051630	4.350330
254.877121	6492.010950	8.295104	-0.051693	4.352957
254.833389	6500.068912	8.300109	-0.051691	4.355563
254.941444	6508.031331	8.305114	-0.051716	4.358138
255.248306	6515.952362	8.310118	-0.051778	4.360699
255.181881	6523.997091	8.315123	-0.051771	4.363296
255.394035	6531.993247	8.320128	-0.051816	4.365878
255.545104	6539.956572	8.325133	-0.051850	4.368447
255.968899	6548.024547	8.330138	-0.051934	4.371050
255.771066	6556.090759	8.335142	-0.051902	4.373647
256.156293	6564.092598	8.340147	-0.051979	4.376225
256.335219	6572.121231	8.345152	-0.052018	4.378809
256.622138	6580.066453	8.350157	-0.052077	4.381366
256.860338	6588.113446	8.355162	-0.052126	4.383953
256.944162	6596.150299	8.360166	-0.052147	4.386534
257.211292	6604.113099	8.365171	-0.052202	4.389092
257.344170	6612.206422	8.370176	-0.052232	4.391688
257.442804	6620.218436	8.375181	-0.052256	4.394258
257.774017	6628.270584	8.380186	-0.052323	4.396839
257.832103	6636.198157	8.385190	-0.052339	4.399378
258.086066	6644.255227	8.390195	-0.052392	4.401958
258.095154	6652.244610	8.395200	-0.052399	4.404513
258.222729	6660.274033	8.400205	-0.052428	4.407080
258.292579	6668.306099	8.405210	-0.052446	4.409647
258.416159	6676.353850	8.410214	-0.052475	4.412217
259.045591	6684.360090	8.415219	-0.052597	4.414774
259.295465	6692.402936	8.420224	-0.052649	4.417340
259.312379	6700.379284	8.425229	-0.052657	4.419882
259.787522	6708.455048	8.430234	-0.052751	4.422457
259.845890	6716.406852	8.435238	-0.052767	4.424988
259.926259	6724.405161	8.440243	-0.052788	4.427533
260.220459	6732.425982	8.445248	-0.052848	4.430085
260.414623	6740.501957	8.450253	-0.052889	4.432652
260.794712	6748.542030	8.455258	-0.052965	4.435207
260.873633	6756.542393	8.460262	-0.052985	4.437747
261.080645	6764.518266	8.465267	-0.053029	4.440278
261.322581	6772.568298	8.470272	-0.053080	4.442831
261.393392	6780.497931	8.475277	-0.053098	4.445344
261.543612	6788.591910	8.480282	-0.053131	4.447908
261.833054	6796.527235	8.485286	-0.053190	4.450421
261.861467	6804.609273	8.490291	-0.053201	4.452977
262.100270	6812.641322	8.495296	-0.053251	4.455517
262.282885	6820.649009	8.500301	-0.053290	4.458048
262.379751	6828.634538	8.505306	-0.053314	4.460570
262.531657	6836.703226	8.510310	-0.053347	4.463117
262.931855	6844.664176	8.515315	-0.053427	4.465629
263.052634	6852.703879	8.520320	-0.053455	4.468164
263.109074	6860.720085	8.525325	-0.053471	4.470689
263.267415	6868.776579	8.530330	-0.053505	4.473227
263.455651	6876.779881	8.535334	-0.053546	4.475746
263.402425	6884.810836	8.540339	-0.053541	4.478272
263.716733	6892.790367	8.545344	-0.053605	4.480781
263.864392	6900.769997	8.550349	-0.053638	4.483288
264.113721	6908.781140	8.555354	-0.053690	4.485804
264.205198	6916.802188	8.560359	-0.053712	4.488321
264.196304	6924.801719	8.565363	-0.053716	4.490830
264.519887	6932.885770	8.570368	-0.053781	4.493365
264.619800	6940.846669	8.575373	-0.053805	4.495859
264.972497	6948.890912	8.580378	-0.053876	4.498379
265.136319	6956.893303	8.585383	-0.053912	4.500883
265.353151	6964.907832	8.590387	-0.053958	4.503390
265.486242	6972.910522	8.595392	-0.053988	4.505892
265.612254	6980.944758	8.600397	-0.054016	4.508402
265.857872	6988.960736	8.605402	-0.054067	4.510905
266.173789	6997.026860	8.610407	-0.054132	4.513423
266.484104	7005.046586	8.615411	-0.054195	4.515924
266.508230	7013.073610	8.620416	-0.054205	4.518426
266.709250	7021.009841	8.625421	-0.054247	4.520899
266.958448	7029.058560	8.630426	-0.054299	4.523405
267.328244	7037.007827	8.635431	-0.054373	4.525879
267.267163	7045.045182	8.640435	-0.054367	4.528379
267.437671	7053.053648	8.645440	-0.054404	4.530868
267.592530	7061.116933	8.650445	-0.054438	4.533373
268.032772	7069.134142	8.655450	-0.054526	4.535863
268.052934	7077.140690	8.660455	-0.054535	4.538348
268.407940	7085.124043	8.665459	-0.054606	4.540824
268.840056	7093.180102	8.670464	-0.054692	4.543322
268.791732	7101.127697	8.675469	-0.054688	4.545784
268.983773	7109.211852	8.680474	-0.054729	4.548287
269.166949	7117.193602	8.685479	-0.054769	4.550757
269.275308	7125.226459	8.690483	-0.054794	4.553241
269.620503	7133.303444	8.695488	-0.054864	4.555738
269.505762	7141.259962	8.700493	-0.054848	4.558196
269.819418	7149.283315	8.705498	-0.054911	4.560674
269.854035	7157.306791	8.710503	-0.054923	4.563150
270.002266	7165.287814	8.715507	-0.054956	4.565612
270.166328	7173.371444	8.720512	-0.054992	4.568104
270.202082	7181.294584	8.725517	-0.055004	4.570545
270.518550	7189.397972	8.730522	-0.055068	4.573040
270.624704	7197.394613	8.735527	-0.055093	4.575501
270.861606	7205.430975	8.740531	-0.055143	4.577973
271.126280	7213.444326	8.745536	-0.055197	4.580437
271.438469	7221.437667	8.750541	-0.055261	4.582893
271.791155	7229.425230	8.755546	-0.055332	4.585346
271.717219	7237.482546	8.760551	-0.055323	4.587819
271.813650	7245.435209	8.765555	-0.055347	4.590258
272.183524	7253.541851	8.770560	-0.055421	4.592744
272.241229	7261.608167	8.775565	-0.055437	4.595216
272.381609	7269.616680	8.780570	-0.055468	4.597668
272.490806	7277.567283	8.785575	-0.055494	4.600102
272.800785	7285.578426	8.790579	-0.055557	4.602553
272.857762	7293.545744	8.795584	-0.055573	4.604989
273.170070	7301.579920	8.800589	-0.055636	4.607444
273.367074	7309.555998	8.805594	-0.055678	4.609880
273.682083	7317.641919	8.810599	-0.055742	4.612348
273.721079	7325.641773	8.815603	-0.055755	4.614789
274.016900	7333.693472	8.820608	-0.055815	4.617244
274.043845	7341.633245	8.825613	-0.055826	4.619664
274.160042	7349.709645	8.830618	-0.055853	4.622124
274.471245	7357.678053	8.835623	-0.055916	4.624550
274.577697	7365.724122	8.840627	-0.055941	4.626998
274.570633	7373.747482	8.845632	-0.055945	4.629438
274.554945	7381.734989	8.850637	-0.055947	4.631866
274.927486	7389.865683	8.855642	-0.056022	4.634336
274.888354	7397.814335	8.860647	-0.056020	4.636750
274.842832	7405.770185	8.865651	-0.056017	4.639164
275.093320	7413.809545	8.870656	-0.056069	4.641603
275.166822	7421.793813	8.875661	-0.056088	4.644023
275.268046	7429.791676	8.880666	-0.056112	4.646446
275.460741	7437.868408	8.885671	-0.056153	4.648892
275.519428	7445.848785	8.890675	-0.056169	4.651308
275.940494	7453.903211	8.895680	-0.056253	4.653744
275.927938	7461.893762	8.900685	-0.056256	4.656160
276.127720	7469.914370	8.905690	-0.056299	4.658583
276.135625	7477.912359	8.910695	-0.056305	4.660999
276.242501	7485.897477	8.915699	-0.056331	4.663410
276.482486	7493.936189	8.920704	-0.056381	4.665835
276.576704	7501.996951	8.925709	-0.056404	4.668266
276.921990	7510.047972	8.930714	-0.056473	4.670692
276.833016	7518.090185	8.935719	-0.056462	4.673115
277.294116	7526.098680	8.940723	-0.056553	4.675525
277.447867	7534.134317	8.945728	-0.056587	4.677943
277.598053	7542.005966	8.950733	-0.056620	4.680311
277.822927	7550.050475	8.955738	-0.056667	4.682729
277.779357	7558.047377	8.960743	-0.056665	4.685132
277.989740	7566.055494	8.965747	-0.056709	4.687536
278.119476	7574.066147	8.970752	-0.056739	4.689941
278.414905	7582.124963	8.975757	-0.056799	4.692358
278.456697	7590.156830	8.980762	-0.056812	4.694766
278.550812	7598.179738	8.985767	-0.056835	4.697170
278.829740	7606.117681	8.990771	-0.056892	4.699547
279.084866	7614.224352	8.995776	-0.056945	4.701974
279.177568	7622.127237	9.000781	-0.056967	4.704338
279.350260	7630.185224	9.005786	-0.057005	4.706748
279.580996	7638.209305	9.010791	-0.057053	4.709146
279.630336	7646.263022	9.015795	-0.057068	4.711552
279.811697	7654.291839	9.020800	-0.057107	4.713949
279.648574	7662.269093	9.025805	-0.057082	4.716331
279.875228	7670.306605	9.030810	-0.057129	4.718728
280.148351	7678.323643	9.035815	-0.057186	4.721117
280.425194	7686.326034	9.040819	-0.057242	4.723501
280.738073	7694.339260	9.045824	-0.057306	4.725887
280.591966	7702.379983	9.050829	-0.057284	4.728281
281.022415	7710.388102	9.055834	-0.057370	4.730663
281.283954	7718.436325	9.060839	-0.057424	4.733055
281.135287	7726.385264	9.065843	-0.057401	4.735419
281.362698	7734.476007	9.070848	-0.057449	4.737822
281.540908	7742.454692	9.075853	-0.057487	4.740190
281.805138	7750.490039	9.080858	-0.057542	4.742574
281.771374	7758.424823	9.085863	-0.057541	4.744928
281.864172	7766.494666	9.090867	-0.057563	4.747321
282.228550	7774.502517	9.095872	-0.057637	4.749693
282.217659	7782.526560	9.100877	-0.057640	4.752069
282.357965	7790.593517	9.105882	-0.057671	4.754457
282.786640	7798.621982	9.110887	-0.057757	4.756831
282.876437	7806.553986	9.115891	-0.057779	4.759177
282.987308	7814.580027	9.120896	-0.057804	4.761549
283.102796	7822.544656	9.125901	-0.057831	4.763901
283.171626	7830.546457	9.130906	-0.057849	4.766264
283.486594	7838.613958	9.135911	-0.057913	4.768644
283.753669	7846.600247	9.140915	-0.057968	4.770999
284.025320	7854.685974	9.145920	-0.058024	4.773382
284.058195	7862.690725	9.150925	-0.058036	4.775741
284.194301	7870.655422	9.155930	-0.058066	4.778087
284.544768	7878.685691	9.160935	-0.058137	4.780449
284.672201	7886.702841	9.165939	-0.058166	4.782808
284.881651	7894.715732	9.170944	-0.058210	4.785164
284.946955	7902.751626	9.175949	-0.058228	4.787526
285.363956	7910.739764	9.180954	-0.058311	4.789871
285.475122	7918.794016	9.185959	-0.058337	4.792236
285.569952	7926.814795	9.190963	-0.058360	4.794590
285.836201	7934.849858	9.195968	-0.058415	4.796946
285.936567	7942.793551	9.200973	-0.058439	4.799275
285.902553	7950.814508	9.205978	-0.058438	4.801626
286.281106	7958.807046	9.210983	-0.058513	4.803966
286.395476	7966.806504	9.215987	-0.058540	4.806308
286.548713	7974.899159	9.220992	-0.058574	4.808676
286.626253	7982.882436	9.225997	-0.058594	4.811011
286.780450	7990.236612	9.231002	-0.058627	4.813160
287.057257	7994.738453	9.236007	-0.058682	4.814474

287.102405	7997.193312	9.241011	-0.058692	4.815192
287.203096	7998.576708	9.246016	-0.058712	4.815595
287.227534	7998.999239	9.251021	-0.058717	4.815719
287.286550	8000.036863	9.256026	-0.058728	4.816021
287.523599	8000.029433	9.261031	-0.058773	4.816018
287.576856	7999.972705	9.266035	-0.058783	4.816001
287.543514	7999.994548	9.271040	-0.058776	4.816008
287.564867	8000.018456	9.276045	-0.058780	4.816015
287.776060	7999.973153	9.281050	-0.058820	4.816000
287.717712	8000.028737	9.286055	-0.058809	4.816017
287.792521	7999.989500	9.291059	-0.058823	4.816005
287.957373	8000.040600	9.296064	-0.058854	4.816019
287.767173	8000.012567	9.301069	-0.058819	4.816012
287.842862	7999.969071	9.306074	-0.058833	4.815999
287.932113	8000.002764	9.311079	-0.058850	4.816008
288.037325	7999.944845	9.316083	-0.058869	4.815990
288.076661	8000.010758	9.321088	-0.058877	4.816010
288.101184	7999.944957	9.326093	-0.058881	4.815990
288.258696	7999.922186	9.331098	-0.058911	4.815983
288.244568	8000.038421	9.336103	-0.058908	4.816017
288.294289	7999.996590	9.341107	-0.058917	4.816004
288.525219	8000.015766	9.346112	-0.058961	4.816009
288.459143	7999.988923	9.351117	-0.058948	4.816001
288.549498	7999.984166	9.356122	-0.058965	4.815999
288.455421	8000.052993	9.361127	-0.058948	4.816020
288.438815	7999.986443	9.366131	-0.058945	4.816000
288.563039	8000.020774	9.371136	-0.058968	4.816010
288.508987	8000.031554	9.376141	-0.058958	4.816013
288.565818	8000.031529	9.381146	-0.058969	4.816013
288.714993	8000.100513	9.386151	-0.058997	4.816032
288.590532	8000.040546	9.391155	-0.058974	4.816015
288.693731	8000.056328	9.396160	-0.058993	4.816020
288.644817	8000.043691	9.401165	-0.058984	4.816016
288.840722	8000.047268	9.406170	-0.059020	4.816016
288.788542	8000.047395	9.411175	-0.059011	4.816016
288.796194	7999.988767	9.416179	-0.059012	4.815999
289.006923	8000.046048	9.421184	-0.059052	4.816015
288.915526	8000.030499	9.426189	-0.059035	4.816011
288.882341	7999.977539	9.431194	-0.059029	4.815995
288.922710	8000.062708	9.436199	-0.059036	4.816020
288.893492	7999.969210	9.441203	-0.059031	4.815993
289.123434	8000.031117	9.446208	-0.059074	4.816010
288.957422	8000.008865	9.451213	-0.059043	4.816004
288.847990	8000.078482	9.456218	-0.059023	4.816025
288.928544	8000.089576	9.461223	-0.059038	4.816028
289.092231	8000.054095	9.466227	-0.059068	4.816017
289.224868	8000.087512	9.471232	-0.059093	4.816026
289.154016	8000.047758	9.476237	-0.059080	4.816015
288.931654	8000.016999	9.481242	-0.059039	4.816007
289.166275	8000.074716	9.486247	-0.059083	4.816022
289.089245	8000.026300	9.491251	-0.059068	4.816009
289.037139	8000.042458	9.496256	-0.059059	4.816014
289.060618	8000.012972	9.501261	-0.059063	4.816005
289.092244	8000.065922	9.506266	-0.059069	4.816020
289.177910	8000.046118	9.511271	-0.059085	4.816014
289.217496	8000.010513	9.516275	-0.059093	4.816003
289.136967	8000.056077	9.521280	-0.059078	4.816017
289.303386	8000.040951	9.526285	-0.059109	4.816012
289.164988	8000.077979	9.531290	-0.059083	4.816023
289.221872	8000.062994	9.536295	-0.059094	4.816019
289.129632	8000.033537	9.541299	-0.059077	4.816010
289.230878	8000.083481	9.546304	-0.059096	4.816025
289.064304	8000.049463	9.551309	-0.059065	4.816015
289.043305	8000.085425	9.556314	-0.059061	4.816026
289.234846	8000.108160	9.561319	-0.059097	4.816032
289.248733	8000.034683	9.566323	-0.059099	4.816010
289.435391	8000.075497	9.571328	-0.059134	4.816021
289.357587	8000.083706	9.576333	-0.059120	4.816024
289.529447	8000.048374	9.581338	-0.059152	4.816013
289.510248	8000.064064	9.586343	-0.059148	4.816017
289.418682	8000.059198	9.591347	-0.059131	4.816016
289.596782	8000.105200	9.596352	-0.059165	4.816029
289.663478	8000.093600	9.601357	-0.059177	4.816025
289.554360	8000.043529	9.606362	-0.059157	4.816011
289.551321	8000.112948	9.611367	-0.059157	4.816031
289.616654	8000.056438	9.616371	-0.059169	4.816015
289.414213	8000.075201	9.621376	-0.059131	4.816021
289.317105	8000.029624	9.626381	-0.059113	4.816008
289.561385	8000.044771	9.631386	-0.059159	4.816011
289.685541	8000.045973	9.636391	-0.059182	4.816011
289.536163	8000.053947	9.641395	-0.059154	4.816014
289.661977	8000.082966	9.646400	-0.059178	4.816022
289.645413	8000.086948	9.651405	-0.059175	4.816023
289.455774	8000.025792	9.656410	-0.059140	4.816006
289.560605	8000.039467	9.661415	-0.059159	4.816010
289.584810	8000.012131	9.666419	-0.059164	4.816002
289.630193	8000.034341	9.671424	-0.059172	4.816008
289.688417	8000.055716	9.676429	-0.059183	4.816014
289.510701	8000.016151	9.681434	-0.059150	4.816003
289.636890	8000.117848	9.686439	-0.059174	4.816032
289.548000	8000.067077	9.691443	-0.059157	4.816018
289.735579	8000.076916	9.696448	-0.059192	4.816020
289.782395	8000.056404	9.701453	-0.059201	4.816014
289.715234	8000.040228	9.706458	-0.059189	4.816009
289.687880	8000.065387	9.711463	-0.059184	4.816017
289.653962	8000.012412	9.716467	-0.059178	4.816001
289.855870	8000.089840	9.721472	-0.059215	4.816023
289.758174	8000.069901	9.726477	-0.059197	4.816018
289.737194	8000.010749	9.731482	-0.059193	4.816000
289.721142	8000.055351	9.736487	-0.059190	4.816014
289.760039	8000.021870	9.741491	-0.059198	4.816004
289.763093	8000.049721	9.746496	-0.059198	4.816012
289.800684	8000.067514	9.751501	-0.059206	4.816017
289.810720	8000.061294	9.756506	-0.059207	4.816015
290.013796	8000.089584	9.761511	-0.059245	4.816022
289.818978	8000.071081	9.766515	-0.059209	4.816018
290.070248	8000.102387	9.771520	-0.059256	4.816025
289.865180	8000.108276	9.776525	-0.059218	4.816028
289.805552	8000.095443	9.781530	-0.059207	4.816025
290.019271	8000.151714	9.786535	-0.059247	4.816040
289.935987	8000.041197	9.791539	-0.059231	4.816008
289.891115	8000.033976	9.796544	-0.059223	4.816006
289.712858	8000.044629	9.801549	-0.059190	4.816010
289.808707	8000.027148	9.806554	-0.059208	4.816005
289.931104	8000.089235	9.811559	-0.059231	4.816022
289.726283	8000.002153	9.816563	-0.059193	4.815998
289.845702	8000.069529	9.821568	-0.059215	4.816017
289.817820	8000.005976	9.826573	-0.059210	4.815999
289.776859	8000.004170	9.831578	-0.059203	4.815998
290.064101	8000.042543	9.836583	-0.059256	4.816008
289.898807	8000.054502	9.841587	-0.059225	4.816012
289.961757	8000.050314	9.846592	-0.059237	4.816011
290.070678	8000.003148	9.851597	-0.059258	4.815996
290.086567	8000.038714	9.856602	-0.059261	4.816007
289.927613	8000.080711	9.861607	-0.059231	4.816020
289.838367	7999.996804	9.866611	-0.059215	4.815996
289.948995	8000.090737	9.871616	-0.059235	4.816023
289.950981	8000.064065	9.876621	-0.059236	4.816015
289.977611	8000.047460	9.881626	-0.059241	4.816010
290.034057	8000.112620	9.886631	-0.059251	4.816029
289.932649	8000.060551	9.891635	-0.059233	4.816014
290.097594	8000.069979	9.896640	-0.059263	4.816016
290.083739	8000.033399	9.901645	-0.059261	4.816005
290.053061	7999.982620	9.906650	-0.059255	4.815990
289.993471	8000.041390	9.911655	-0.059244	4.816008
290.111594	7999.984774	9.916659	-0.059266	4.815991
290.169874	8000.094853	9.921664	-0.059277	4.816023
290.268208	8000.130853	9.926669	-0.059296	4.816033
290.148874	8000.020747	9.931674	-0.059274	4.816001
290.307153	8000.085626	9.936679	-0.059303	4.816019
290.201539	8000.067679	9.941683	-0.059284	4.816015
290.132091	8000.098484	9.946688	-0.059271	4.816024
290.088795	8000.105184	9.951693	-0.059263	4.816026
290.170546	8000.081034	9.956698	-0.059278	4.816019
290.407303	8000.097115	9.961703	-0.059322	4.816022
290.190776	8000.053635	9.966707	-0.059282	4.816010
290.184177	8000.047111	9.971712	-0.059281	4.816009
290.339036	8000.063836	9.976717	-0.059310	4.816013
290.204886	8000.069949	9.981722	-0.059285	4.816015
290.410185	8000.091869	9.986727	-0.059323	4.816020
290.312635	8000.075137	9.991731	-0.059305	4.816016
290.118992	8000.065204	9.996736	-0.059269	4.816014
290.197858	8000.034590	10.001741	-0.059284	4.816005
290.350929	8000.053419	10.006746	-0.059313	4.816010
290.383842	8000.082884	10.011751	-0.059319	4.816018
290.107684	8000.047935	10.016755	-0.059268	4.816009
290.314569	8000.020722	10.021760	-0.059306	4.816000
290.396901	8000.085286	10.026765	-0.059322	4.816019
290.253002	8000.009999	10.031770	-0.059295	4.815997
290.306625	8000.072971	10.036775	-0.059305	4.816015
290.371428	7999.996145	10.041779	-0.059317	4.815993
290.349657	7999.982933	10.046784	-0.059313	4.815989
290.166145	8000.080056	10.051789	-0.059279	4.816018
290.207449	8000.010283	10.056794	-0.059287	4.815998
290.236014	8000.039667	10.061799	-0.059292	4.816006
290.184948	7999.983173	10.066803	-0.059283	4.815990
290.349556	8000.028930	10.071808	-0.059314	4.816002
290.163226	8000.047986	10.076813	-0.059279	4.816009
290.171923	7999.923115	10.081818	-0.059281	4.815972
290.398845	8000.069398	10.086823	-0.059323	4.816014
290.349344	8000.059955	10.091827	-0.059314	4.816011
290.493814	8000.035879	10.096832	-0.059341	4.816004
290.300325	8000.019537	10.101837	-0.059305	4.816000
290.347485	8000.027886	10.106842	-0.059314	4.816002
290.472136	8000.015206	10.111847	-0.059337	4.815998
290.396363	8000.056582	10.116851	-0.059323	4.816010
290.323378	8000.072360	10.121856	-0.059310	4.816015
290.424384	8000.048561	10.126861	-0.059329	4.816008
290.271751	8000.013726	10.131866	-0.059300	4.815998
290.395548	8000.072634	10.136871	-0.059323	4.816015
290.297156	8000.004589	10.141875	-0.059305	4.815995
290.435081	8000.001768	10.146880	-0.059331	4.815994
290.322790	8000.005074	10.151885	-0.059310	4.815995
290.329959	7999.979565	10.156890	-0.059311	4.815988
290.407819	7999.997023	10.161895	-0.059326	4.815993
290.219479	7999.998943	10.166899	-0.059291	4.815994
290.360405	8000.111598	10.171904	-0.059317	4.816026
290.455918	8000.100524	10.176909	-0.059335	4.816023
290.235622	8000.063387	10.181914	-0.059294	4.816013
290.328975	8000.107846	10.186919	-0.059312	4.816025
290.467913	8000.077257	10.191923	-0.059338	4.816016
290.431544	8000.006068	10.196928	-0.059331	4.815995
290.307274	8000.026255	10.201933	-0.059308	4.816002
290.353271	8000.037789	10.206938	-0.059317	4.816005
290.732908	8000.137698	10.211943	-0.059388	4.816032
290.370241	7999.953688	10.216947	-0.059320	4.815980
290.562651	8000.035221	10.221952	-0.059356	4.816003
290.447127	8000.034192	10.226957	-0.059335	4.816003
290.763963	7999.970510	10.231962	-0.059394	4.815983
290.594987	8000.046524	10.236967	-0.059362	4.816006
290.444097	7999.977522	10.241971	-0.059334	4.815987
290.618685	7999.986057	10.246976	-0.059367	4.815988
290.425761	8000.070184	10.251981	-0.059331	4.816014
290.495009	7999.988095	10.256986	-0.059344	4.815990
290.580039	8000.060190	10.261991	-0.059360	4.816010
290.556641	8000.062978	10.266995	-0.059356	4.816011
290.648969	8000.041159	10.272000	-0.059373	4.816004
290.720496	8000.018960	10.277005	-0.059386	4.815997
290.627531	7999.972388	10.282010	-0.059369	4.815984
290.638009	8000.027092	10.287015	-0.059371	4.816000
290.609678	8000.016966	10.292019	-0.059366	4.815997
290.700576	8000.044282	10.297024	-0.059383	4.816005
290.682174	8000.086704	10.302029	-0.059380	4.816017
290.581870	7999.988700	10.307034	-0.059361	4.815989
290.704967	8000.082862	10.312039	-0.059384	4.816016
290.619319	8000.056729	10.317043	-0.059368	4.816009
290.472695	8000.041241	10.322048	-0.059341	4.816005
290.659783	8000.063897	10.327053	-0.059376	4.816011
290.509822	8000.006668	10.332058	-0.059348	4.815995
290.749404	8000.083717	10.337063	-0.059393	4.816016
290.875638	8000.045416	10.342067	-0.059416	4.816004
290.903765	8000.042732	10.347072	-0.059422	4.816003
290.744634	8000.052664	10.352077	-0.059392	4.816007
290.623212	7999.992749	10.357082	-0.059370	4.815990
290.876338	8000.070046	10.362087	-0.059417	4.816011
290.763527	8000.072273	10.367091	-0.059396	4.816013
290.678788	8000.055775	10.372096	-0.059380	4.816008
290.991609	8000.068968	10.377101	-0.059439	4.816010
290.831666	8000.048961	10.382106	-0.059409	4.816005
290.641976	8000.055130	10.387111	-0.059374	4.816008
290.702160	8000.062649	10.392115	-0.059385	4.816010
290.856813	8000.040897	10.397120	-0.059414	4.816003
290.701432	8000.064791	10.402125	-0.059385	4.816011
290.532923	8000.029666	10.407130	-0.059354	4.816001
290.810413	8000.122370	10.412135	-0.059406	4.816027
290.761780	8000.066987	10.417139	-0.059397	4.816011
290.805187	8000.047481	10.422144	-0.059405	4.816005
290.756853	8000.086152	10.427149	-0.059396	4.816017
290.872189	7999.995284	10.432154	-0.059417	4.815990
290.795814	8000.103980	10.437159	-0.059403	4.816022
290.759272	8000.044542	10.442163	-0.059397	4.816005
290.847898	8000.039755	10.447168	-0.059413	4.816003
290.890231	8000.095041	10.452173	-0.059421	4.816019
290.721633	7999.995791	10.457178	-0.059390	4.815990
290.660788	8000.068432	10.462183	-0.059379	4.816012
290.664945	8000.042868	10.467187	-0.059380	4.816005
290.757232	8000.010360	10.472192	-0.059397	4.815995
290.807547	8000.090372	10.477197	-0.059406	4.816018
290.898991	8000.043955	10.482202	-0.059423	4.816004
290.988976	8000.085148	10.487207	-0.059440	4.816015
290.885480	8000.090751	10.492211	-0.059421	4.816017
290.774450	8000.093010	10.497216	-0.059400	4.816019
290.954948	8000.097379	10.502221	-0.059434	4.816019
290.754165	8000.046703	10.507226	-0.059397	4.816005
291.028975	8000.148977	10.512231	-0.059448	4.816034
291.092755	8000.079613	10.517235	-0.059460	4.816013
290.904431	8000.069775	10.522240	-0.059425	4.816011
290.794812	8000.065648	10.527245	-0.059405	4.816010
290.916517	8000.056120	10.532250	-0.059428	4.816007
290.869123	8000.095877	10.537255	-0.059419	4.816019
290.835021	8000.072821	10.542259	-0.059413	4.816012
291.072055	8000.062189	10.547264	-0.059457	4.816008
290.889079	8000.118711	10.552269	-0.059423	4.816025
290.773146	8000.047139	10.557274	-0.059401	4.816005
290.949296	8000.103796	10.562279	-0.059434	4.816021
291.034131	8000.036953	10.567283	-0.059450	4.816001
290.747939	8000.054187	10.572288	-0.059397	4.816007
290.702349	8000.095045	10.577293	-0.059389	4.816020
291.014066	8000.079363	10.582298	-0.059447	4.816013
291.018956	8000.151066	10.587303	-0.059448	4.816034
290.805015	8000.094806	10.592307	-0.059408	4.816019
290.916975	8000.040214	10.597312	-0.059429	4.816002
290.902338	8000.107286	10.602317	-0.059426	4.816022
290.741332	8000.054129	10.607322	-0.059396	4.816007
291.029682	8000.112832	10.612327	-0.059450	4.816023
290.956566	8000.038834	10.617331	-0.059437	4.816002
290.910875	8000.011292	10.622336	-0.059428	4.815994
290.850876	8000.096774	10.627341	-0.059417	4.816019
290.820476	8000.064167	10.632346	-0.059411	4.816010
290.917923	8000.076640	10.637351	-0.059430	4.816013
291.036814	8000.092710	10.642355	-0.059452	4.816017
291.008102	8000.049446	10.647360	-0.059447	4.816005
291.135596	8000.062467	10.652365	-0.059471	4.816008
290.901622	8000.071035	10.657370	-0.059427	4.816011
290.911471	8000.125729	10.662375	-0.059429	4.816027
291.002582	8000.069687	10.667379	-0.059446	4.816010
291.064181	8000.039826	10.672384	-0.059458	4.816001
290.998468	8000.036499	10.677389	-0.059445	4.816001
291.121988	8000.002424	10.682394	-0.059469	4.815990
291.138394	8000.062581	10.687399	-0.059472	4.816008
290.986475	8000.010658	10.692403	-0.059443	4.815993
291.081235	8000.034838	10.697408	-0.059461	4.816000
291.041980	8000.009551	10.702413	-0.059454	4.815993
290.858584	8000.021178	10.707418	-0.059420	4.815997
290.977116	8000.147321	10.712423	-0.059442	4.816033
290.998028	8000.087862	10.717427	-0.059446	4.816016
290.927678	8000.114375	10.722432	-0.059433	4.816024
290.803950	8000.129228	10.727437	-0.059410	4.816029
290.986072	8000.006448	10.732442	-0.059444	4.815992
291.076450	8000.085053	10.737447	-0.059461	4.816015
291.074574	8000.061516	10.742451	-0.059461	4.816008
290.992926	8000.052555	10.747456	-0.059446	4.816005
291.152751	8000.102502	10.752461	-0.059476	4.816019
290.986922	8000.080250	10.757466	-0.059445	4.816014
291.111853	8000.092156	10.762471	-0.059468	4.816016
291.039388	8000.056644	10.767475	-0.059455	4.816006
291.028991	8000.065013	10.772480	-0.059453	4.816009
290.973734	8000.060808	10.777485	-0.059443	4.816008
291.235105	8000.117951	10.782490	-0.059491	4.816023
291.135823	8000.132181	10.787495	-0.059473	4.816028
290.838561	8000.101120	10.792499	-0.059418	4.816020
290.925496	8000.048209	10.797504	-0.059434	4.816005
291.142265	8000.078888	10.802509	-0.059475	4.816012
291.085840	8000.056494	10.807514	-0.059464	4.816006
291.217818	8000.053566	10.812519	-0.059489	4.816005
291.221571	8000.016237	10.817523	-0.059490	4.815994
291.124407	7999.994169	10.822528	-0.059472	4.815988
291.163334	8000.049393	10.827533	-0.059479	4.816004
290.887640	8000.053993	10.832538	-0.059428	4.816006
291.055773	8000.088061	10.837543	-0.059459	4.816015
291.234097	8000.077428	10.842547	-0.059492	4.816011
291.188375	7999.968661	10.847552	-0.059484	4.815980
291.309489	8000.000803	10.852557	-0.059507	4.815989
291.046654	8000.021669	10.857562	-0.059458	4.815996
291.209409	8000.027852	10.862567	-0.059488	4.815997
291.047670	8000.004606	10.867571	-0.059458	4.815991
291.144297	7999.981796	10.872576	-0.059476	4.815984
291.132961	8000.063891	10.877581	-0.059474	4.816008
290.962525	8000.070411	10.882586	-0.059443	4.816011
291.101321	8000.028063	10.887591	-0.059468	4.815998
290.999124	7999.969566	10.892595	-0.059449	4.815981
290.937471	7999.973795	10.897600	-0.059438	4.815983
291.062604	8000.032728	10.902605	-0.059461	4.815999
291.178887	8000.000658	10.907610	-0.059483	4.815989
291.144887	8000.090889	10.912615	-0.059477	4.816016
291.137637	8000.030917	10.917619	-0.059476	4.815998
291.300995	8000.007186	10.922624	-0.059506	4.815990
291.249809	8000.082142	10.927629	-0.059497	4.816013
291.043401	8000.051669	10.932634	-0.059458	4.816005
291.125871	8000.069213	10.937639	-0.059474	4.816010
291.291187	8000.070099	10.942643	-0.059505	4.816009
291.107764	8000.051801	10.947648	-0.059471	4.816005
291.104081	7999.945938	10.952653	-0.059470	4.815974
290.987363	7999.859390	10.957658	-0.059448	4.815949
291.211220	7999.975696	10.962663	-0.059490	4.815982
291.132850	7999.988170	10.967667	-0.059476	4.815986
291.208011	7999.945731	10.972672	-0.059490	4.815973
291.359832	8000.074619	10.977677	-0.059518	4.816010
291.360295	7999.996619	10.982682	-0.059518	4.815987
291.343655	8000.104267	10.987687	-0.059515	4.816019
291.240084	8000.071394	10.992691	-0.059496	4.816010
291.084400	8000.002302	10.997696	-0.059467	4.815990
291.291062	8000.106541	11.002701	-0.059506	4.816020
291.251552	8000.049186	11.007706	-0.059499	4.816003
291.371383	8000.051380	11.012711	-0.059521	4.816003
291.230601	8000.073403	11.017715	-0.059495	4.816010
291.348268	7999.990059	11.022720	-0.059517	4.815985
291.388850	8000.051726	11.027725	-0.059525	4.816003
291.328177	8000.007879	11.032730	-0.059513	4.815990
291.571645	7999.970646	11.037735	-0.059559	4.815978
291.528139	8000.067118	11.042739	-0.059551	4.816007
291.505987	8000.013285	11.047744	-0.059547	4.815991
291.446453	8000.100914	11.052749	-0.059536	4.816017
291.445059	8000.014330	11.057754	-0.059536	4.815992
291.550665	8000.083595	11.062759	-0.059555	4.816011
291.483028	8000.090921	11.067763	-0.059543	4.816014
291.664428	8000.032251	11.072768	-0.059577	4.815996
291.648013	8000.053335	11.077773	-0.059574	4.816002
291.416906	8000.058748	11.082778	-0.059531	4.816005
291.434475	8000.115721	11.087783	-0.059534	4.816021
291.442730	8000.124431	11.092787	-0.059536	4.816024
291.541876	8000.055710	11.097792	-0.059554	4.816003
291.533564	8000.104730	11.102797	-0.059553	4.816018
291.250426	8000.005527	11.107802	-0.059500	4.815990
291.450900	7999.983541	11.112807	-0.059538	4.815983
291.413607	8000.064094	11.117811	-0.059531	4.816006
291.353795	7999.961483	11.122816	-0.059520	4.815977
291.404440	7999.992340	11.127821	-0.059529	4.815985
291.159777	7999.933382	11.132826	-0.059484	4.815970
291.311557	8000.066544	11.137831	-0.059512	4.816008
291.353916	8000.084426	11.142835	-0.059520	4.816013
291.311143	7999.963956	11.147840	-0.059512	4.815978
291.318474	8000.004710	11.152845	-0.059514	4.815990
291.271053	7999.954693	11.157850	-0.059505	4.815975
291.463901	8000.068299	11.162855	-0.059541	4.816007
291.413101	8000.018219	11.167859	-0.059532	4.815993
291.403367	7999.949651	11.172864	-0.059530	4.815973
291.340082	7999.978431	11.177869	-0.059518	4.815982
291.288167	7999.962531	11.182874	-0.059509	4.815977
291.527660	8000.035306	11.187879	-0.059553	4.815997
291.568249	8000.005062	11.192883	-0.059561	4.815988
291.364132	7999.963943	11.197888	-0.059523	4.815977
291.408145	8000.018191	11.202893	-0.059531	4.815993
291.421718	7999.982111	11.207898	-0.059534	4.815982
291.528106	8000.074903	11.212903	-0.059554	4.816009
291.394315	8000.038272	11.217907	-0.059529	4.815999
291.503883	7999.993254	11.222912	-0.059549	4.815985
291.532845	8000.044022	11.227917	-0.059555	4.816000
291.467981	7999.977655	11.232922	-0.059543	4.815981
291.452509	8000.058606	11.237927	-0.059540	4.816005
291.619905	8000.153581	11.242931	-0.059572	4.816031
291.613153	8000.123542	11.247936	-0.059570	4.816023
291.622902	8000.117316	11.252941	-0.059572	4.816021
291.430045	8000.010139	11.257946	-0.059536	4.815990
291.397799	7999.988185	11.262951	-0.059530	4.815984
291.406473	8000.004384	11.267955	-0.059532	4.815989
291.521858	8000.011840	11.272960	-0.059554	4.815990
291.523264	8000.031112	11.277965	-0.059554	4.815996
291.297478	7999.990667	11.282970	-0.059512	4.815985
291.429052	8000.050787	11.287975	-0.059537	4.816002
291.500074	8000.023235	11.292979	-0.059550	4.815994
291.355535	8000.010990	11.297984	-0.059523	4.815991
291.265407	8000.044623	11.302989	-0.059507	4.816001
291.225228	7999.976569	11.307994	-0.059499	4.815982
291.484765	7999.913980	11.312999	-0.059548	4.815962
291.353470	7999.935107	11.318003	-0.059523	4.815969
291.390706	7999.987095	11.323008	-0.059530	4.815984
291.733511	8000.048930	11.328013	-0.059594	4.816000
291.552143	8000.087312	11.333018	-0.059561	4.816012
291.435261	8000.085190	11.338023	-0.059539	4.816012
291.399041	8000.113394	11.343027	-0.059532	4.816021
291.665992	8000.050941	11.348032	-0.059582	4.816001
291.619780	8000.097132	11.353037	-0.059574	4.816015
291.318593	8000.035004	11.358042	-0.059517	4.815998
291.514026	8000.046058	11.363047	-0.059554	4.816000
291.459948	7999.967063	11.368051	-0.059544	4.815978
291.316790	7999.994386	11.373056	-0.059517	4.815986
291.503733	8000.043760	11.378061	-0.059552	4.816000
291.347888	7999.960772	11.383066	-0.059523	4.815976
291.362598	7999.996317	11.388071	-0.059526	4.815987
291.553938	8000.046840	11.393075	-0.059562	4.816000
291.559622	7999.989240	11.398080	-0.059563	4.815984
291.562967	8000.023510	11.403085	-0.059564	4.815994
291.357480	8000.059315	11.408090	-0.059526	4.816005
291.569728	7999.989452	11.413095	-0.059565	4.815984
291.577665	7999.999224	11.418099	-0.059567	4.815986
291.518549	7999.974643	11.423104	-0.059556	4.815980
291.541250	8000.085146	11.428109	-0.059560	4.816012
291.469751	8000.020795	11.433114	-0.059547	4.815993
291.607803	8000.108822	11.438119	-0.059573	4.816018
291.649511	8000.088216	11.443123	-0.059581	4.816012
291.395739	7999.959623	11.448128	-0.059533	4.815976
291.410394	8000.026161	11.453133	-0.059536	4.815995
291.496370	8000.022394	11.458138	-0.059552	4.815994
291.419778	8000.058412	11.463143	-0.059538	4.816005
291.394759	8000.000253	11.468147	-0.059534	4.815988
291.385182	8000.028943	11.473152	-0.059532	4.815996
291.522272	8000.069927	11.478157	-0.059558	4.816007
291.485820	7999.984841	11.483162	-0.059551	4.815983
291.533213	8000.046632	11.488167	-0.059560	4.816000
291.619781	8000.068526	11.493171	-0.059576	4.816006
291.749794	7999.998231	11.498176	-0.059600	4.815985
291.445082	8000.074977	11.503181	-0.059544	4.816009
291.517215	7999.991870	11.508186	-0.059557	4.815985
291.581681	8000.063592	11.513191	-0.059569	4.816005
291.500410	8000.073875	11.518195	-0.059554	4.816009
291.498763	8000.000111	11.523200	-0.059554	4.815987
291.689511	8000.054898	11.528205	-0.059590	4.816002
291.521111	8000.041148	11.533210	-0.059558	4.815999
291.410006	8000.027375	11.538215	-0.059538	4.815995
291.436936	8000.044975	11.543219	-0.059543	4.816000
291.532523	7999.990084	11.548224	-0.059561	4.815984
291.415551	8000.103384	11.553229	-0.059539	4.816018
291.364182	8000.058637	11.558234	-0.059530	4.816005
291.572145	8000.067783	11.563239	-0.059568	4.816006
291.604228	8000.072652	11.568243	-0.059575	4.816008
291.444483	7999.981042	11.573248	-0.059545	4.815982
291.587146	8000.069152	11.578253	-0.059572	4.816007
291.580312	8000.032699	11.583258	-0.059570	4.815996
291.509980	8000.061350	11.588263	-0.059557	4.816005
291.438399	8000.087841	11.593267	-0.059544	4.816013
291.547818	8000.055646	11.598272	-0.059565	4.816003
291.528537	8000.124772	11.603277	-0.059561	4.816023
291.426051	7999.991456	11.608282	-0.059542	4.815985
291.561333	7999.980038	11.613287	-0.059567	4.815981
291.684726	8000.064591	11.618291	-0.059590	4.816005
291.615925	7999.962883	11.623296	-0.059578	4.815976
291.568482	8000.001570	11.628301	-0.059569	4.815987
291.557202	7999.970380	11.633306	-0.059567	4.815978
291.553032	8000.033369	11.638311	-0.059566	4.815996
291.607652	8000.029030	11.643315	-0.059577	4.815995
291.744491	8000.014435	11.648320	-0.059602	4.815990
291.807216	8000.059406	11.653325	-0.059614	4.816003
291.613757	8000.049474	11.658330	-0.059578	4.816001
291.761595	8000.081036	11.663335	-0.059606	4.816009
292.000066	8000.049057	11.668339	-0.059650	4.815999
291.889695	8000.012853	11.673344	-0.059630	4.815989
291.937762	8000.039388	11.678349	-0.059639	4.815996
291.884941	7999.975377	11.683354	-0.059629	4.815978
291.670345	8000.046285	11.688359	-0.059589	4.816000
291.824552	8000.024525	11.693363	-0.059618	4.815992
291.753596	7999.962321	11.698368	-0.059605	4.815975
291.909001	8000.017533	11.703373	-0.059634	4.815990
291.802987	8000.016678	11.708378	-0.059614	4.815990
291.838183	8000.015191	11.713383	-0.059621	4.815990
291.743519	8000.019886	11.718387	-0.059603	4.815991
291.565744	7999.982453	11.723392	-0.059570	4.815981
291.711359	8000.050311	11.728397	-0.059597	4.816000
291.913241	8000.008046	11.733402	-0.059635	4.815987
291.883440	8000.051330	11.738407	-0.059630	4.816000
291.799295	8000.104311	11.743411	-0.059614	4.816016
291.993142	7999.999911	11.748416	-0.059650	4.815984
291.819476	8000.105766	11.753421	-0.059618	4.816016
291.717454	8000.056888	11.758426	-0.059599	4.816002
291.863313	8000.070245	11.763431	-0.059626	4.816005
292.083802	8000.033663	11.768435	-0.059667	4.815994
291.833559	8000.034452	11.773440	-0.059621	4.815995
291.691255	8000.050034	11.778445	-0.059595	4.816000
291.736989	7999.986752	11.783450	-0.059603	4.815982
291.718887	8000.018493	11.788455	-0.059600	4.815991
291.778278	8000.043098	11.793459	-0.059611	4.815998
291.911801	8000.040199	11.798464	-0.059636	4.815996
291.839292	8000.077360	11.803469	-0.059623	4.816008
291.644235	8000.007549	11.808474	-0.059586	4.815988
291.932663	8000.013887	11.813479	-0.059640	4.815989
291.893528	8000.081583	11.818483	-0.059633	4.816009
291.841276	7999.967351	11.823488	-0.059623	4.815976
291.987677	8000.020261	11.828493	-0.059651	4.815990
291.895187	8000.017514	11.833498	-0.059634	4.815990
291.907042	8000.030565	11.838503	-0.059636	4.815994
292.057407	8000.036522	11.843507	-0.059664	4.815995
291.973723	8000.002942	11.848512	-0.059648	4.815985
292.130412	8000.043216	11.853517	-0.059678	4.815996
291.991756	8000.064208	11.858522	-0.059652	4.816003
291.921671	8000.052251	11.863527	-0.059639	4.816000
291.790631	8000.083002	11.868531	-0.059615	4.816010
291.756358	8000.011848	11.873536	-0.059608	4.815989
291.883489	8000.061201	11.878541	-0.059632	4.816003
291.753946	8000.001134	11.883546	-0.059608	4.815986
291.716877	8000.054973	11.888551	-0.059601	4.816002
291.822924	8000.087910	11.893555	-0.059621	4.816011
291.704219	7999.992773	11.898560	-0.059599	4.815984
291.926085	8000.079122	11.903565	-0.059641	4.816008
291.719883	8000.072164	11.908570	-0.059602	4.816007
291.682851	8000.003097	11.913575	-0.059595	4.815987
291.923250	7999.989322	11.918579	-0.059640	4.815981
291.805079	7999.950838	11.923584	-0.059618	4.815971
291.889795	8000.000486	11.928589	-0.059634	4.815985
291.843235	7999.973996	11.933594	-0.059626	4.815977
291.927509	8000.074936	11.938599	-0.059641	4.816006
291.814560	8000.079297	11.943603	-0.059621	4.816008
291.712792	7999.965231	11.948608	-0.059602	4.815976
291.917777	8000.046998	11.953613	-0.059640	4.815998
291.701811	7999.977874	11.958618	-0.059600	4.815979
291.754252	8000.019452	11.963623	-0.059610	4.815991
291.700256	8000.074051	11.968627	-0.059600	4.816007
291.875567	8000.040920	11.973632	-0.059632	4.815997
292.055508	8000.084824	11.978637	-0.059666	4.816009
292.061042	8000.077453	11.983642	-0.059667	4.816006
292.087908	8000.068333	11.988647	-0.059672	4.816004
291.944390	8000.093511	11.993651	-0.059646	4.816012
292.059116	8000.042175	11.998656	-0.059667	4.815996
291.981727	8000.118792	12.003661	-0.059653	4.816019
291.906755	8000.088577	12.008666	-0.059639	4.816010
291.991485	8000.081581	12.013671	-0.059655	4.816008
292.179561	8000.091434	12.018675	-0.059690	4.816010
292.209159	8000.035338	12.023680	-0.059695	4.815993
292.000431	8000.068946	12.028685	-0.059657	4.816004
291.893458	8000.057385	12.033690	-0.059637	4.816001
292.039245	8000.068603	12.038695	-0.059664	4.816004
291.954921	8000.060662	12.043699	-0.059649	4.816002
291.888141	8000.010290	12.048704	-0.059636	4.815988
292.085686	8000.054515	12.053709	-0.059673	4.816000
292.087313	8000.033178	12.058714	-0.059673	4.815993
292.167092	8000.003648	12.063719	-0.059688	4.815984
292.134840	8000.058644	12.068723	-0.059682	4.816000
292.102426	8000.009968	12.073728	-0.059676	4.815986
292.103398	7999.973657	12.078733	-0.059677	4.815976
292.034269	8000.003399	12.083738	-0.059664	4.815985
292.118071	7999.999593	12.088743	-0.059680	4.815983
292.104863	8000.062418	12.093747	-0.059677	4.816002
291.927320	7999.996131	12.098752	-0.059644	4.815983
292.062913	8000.060601	12.103757	-0.059670	4.816001
291.901968	8000.027749	12.108762	-0.059640	4.815993
292.030982	8000.070724	12.113767	-0.059664	4.816005
292.003976	8000.056347	12.118771	-0.059659	4.816000
292.025793	7999.970184	12.123776	-0.059663	4.815975
292.110082	8000.051888	12.128781	-0.059679	4.815999
291.979188	8000.115772	12.133786	-0.059655	4.816018
292.066931	8000.041500	12.138791	-0.059671	4.815996
292.078712	8000.113331	12.143795	-0.059673	4.816017
291.886955	8000.013653	12.148800	-0.059638	4.815989
292.054220	8000.056257	12.153805	-0.059669	4.816000
292.232663	7999.988983	12.158810	-0.059702	4.815980
292.222595	8000.015527	12.163815	-0.059701	4.815987
292.156834	8000.100907	12.168819	-0.059688	4.816013
292.147383	7999.981042	12.173824	-0.059687	4.815978
292.080693	8000.017241	12.178829	-0.059674	4.815989
292.018850	8000.031084	12.183834	-0.059663	4.815993
292.161108	8000.077508	12.188839	-0.059690	4.816006
292.121502	8000.137714	12.193843	-0.059682	4.816024
292.023993	8000.034411	12.198848	-0.059664	4.815994
292.063770	8000.101409	12.203853	-0.059672	4.816013
291.963144	8000.095307	12.208858	-0.059653	4.816012
291.914309	8000.030300	12.213863	-0.059644	4.815993
292.115057	8000.079928	12.218867	-0.059682	4.816007
291.899597	8000.068525	12.223872	-0.059642	4.816005
292.079630	8000.100675	12.228877	-0.059675	4.816013
291.973151	8000.067747	12.233882	-0.059655	4.816004
292.156497	8000.051863	12.238887	-0.059690	4.815998
292.197640	8000.110336	12.243891	-0.059697	4.816015
292.054044	8000.060699	12.248896	-0.059671	4.816001
292.287332	8000.087408	12.253901	-0.059714	4.816008
292.385221	8000.093478	12.258906	-0.059733	4.816009
292.164944	8000.043512	12.263911	-0.059692	4.815996
292.135206	8000.135961	12.268915	-0.059686	4.816023
291.959003	8000.046185	12.273920	-0.059653	4.815998
292.152480	8000.137362	12.278925	-0.059690	4.816023
292.046319	8000.073446	12.283930	-0.059670	4.816005
292.131581	8000.116692	12.288935	-0.059686	4.816017
292.324125	8000.152277	12.293939	-0.059722	4.816027
292.129749	8000.082476	12.298944	-0.059686	4.816007
292.158045	8000.181328	12.303949	-0.059691	4.816036
292.033572	8000.117078	12.308954	-0.059668	4.816018
292.116607	8000.092951	12.313959	-0.059684	4.816010
291.985597	8000.152559	12.318963	-0.059659	4.816029
292.210465	8000.077581	12.323968	-0.059701	4.816005
292.210516	8000.109654	12.328973	-0.059701	4.816015
292.107020	8000.100294	12.333978	-0.059682	4.816013
292.252066	8000.143562	12.338983	-0.059709	4.816025
292.231049	8000.192351	12.343987	-0.059705	4.816039
291.995704	8000.143178	12.348992	-0.059662	4.816026
292.130751	8000.146719	12.353997	-0.059687	4.816026
291.989674	8000.066135	12.359002	-0.059661	4.816003
291.871100	8000.105662	12.364007	-0.059639	4.816015
292.176279	8000.131545	12.369011	-0.059696	4.816021
292.061428	8000.080296	12.374016	-0.059674	4.816007
292.119427	8000.113426	12.379021	-0.059685	4.816016
291.960569	8000.097711	12.384026	-0.059656	4.816013
291.988004	8000.015926	12.389031	-0.059661	4.815989
292.010596	8000.045204	12.394035	-0.059665	4.815997
292.112994	8000.020362	12.399040	-0.059684	4.815989
292.299446	8000.097517	12.404045	-0.059719	4.816011
292.246341	8000.009987	12.409050	-0.059709	4.815985
292.288023	8000.011825	12.414055	-0.059717	4.815986
292.137141	8000.105270	12.419059	-0.059689	4.816014
292.144913	7999.982513	12.424064	-0.059691	4.815978
292.262266	8000.116121	12.429069	-0.059713	4.816016
291.938901	8000.065343	12.434074	-0.059653	4.816003
291.961257	8000.079654	12.439079	-0.059657	4.816007
292.097561	8000.113143	12.444083	-0.059682	4.816016
291.986404	8000.069443	12.449088	-0.059662	4.816004
291.979289	8000.083216	12.454093	-0.059661	4.816008
292.108180	8000.026794	12.459098	-0.059685	4.815991
292.102857	8000.007468	12.464103	-0.059684	4.815985
292.069549	7999.929919	12.469107	-0.059678	4.815963
292.038468	7999.942186	12.474112	-0.059672	4.815967
292.263620	8000.047834	12.479117	-0.059714	4.815996
292.174727	8000.020571	12.484122	-0.059697	4.815989
292.080534	8000.047719	12.489127	-0.059680	4.815997
292.283801	8000.081361	12.494131	-0.059718	4.816006
292.098608	8000.014935	12.499136	-0.059684	4.815988
292.216361	8000.101524	12.504141	-0.059706	4.816012
292.160704	8000.114412	12.509146	-0.059695	4.816016
292.249929	8000.020928	12.514151	-0.059712	4.815989
292.162237	8000.047125	12.519155	-0.059696	4.815997
292.195992	8000.000724	12.524160	-0.059702	4.815983
292.160113	8000.066342	12.529165	-0.059696	4.816002
292.081347	7999.990101	12.534170	-0.059681	4.815981
292.001019	8000.022845	12.539175	-0.059666	4.815990
292.139457	8000.068130	12.544179	-0.059692	4.816003
292.134838	8000.079811	12.549184	-0.059691	4.816006
292.143374	8000.075700	12.554189	-0.059693	4.816005
292.224665	8000.055817	12.559194	-0.059708	4.815999
292.418317	8000.059359	12.564199	-0.059744	4.815999
292.236931	8000.125529	12.569203	-0.059711	4.816019
292.045399	7999.991654	12.574208	-0.059675	4.815981
292.208154	8000.139984	12.579213	-0.059705	4.816024
292.206387	8000.107898	12.584218	-0.059705	4.816014
292.123137	8000.047606	12.589223	-0.059690	4.815997
292.128334	8000.099011	12.594227	-0.059691	4.816012
292.133734	8000.070261	12.599232	-0.059692	4.816004
292.191070	8000.105517	12.604237	-0.059703	4.816014
292.175539	8000.091349	12.609242	-0.059700	4.816010
292.275407	8000.078217	12.614247	-0.059719	4.816005
292.178437	8000.060425	12.619251	-0.059701	4.816000
292.055567	8000.017580	12.624256	-0.059678	4.815989
292.300220	8000.142823	12.629261	-0.059724	4.816024
292.396245	8000.194816	12.634266	-0.059742	4.816039
292.138222	8000.083240	12.639271	-0.059694	4.816007
292.136175	8000.108862	12.644275	-0.059693	4.816015
292.273935	8000.055808	12.649280	-0.059719	4.815999
292.466090	8000.052910	12.654285	-0.059755	4.815997
292.339765	8000.128635	12.659290	-0.059731	4.816020
292.320211	8000.133631	12.664295	-0.059728	4.816021
292.290039	8000.163015	12.669299	-0.059722	4.816030
292.062767	8000.068032	12.674304	-0.059680	4.816003
292.327820	8000.083564	12.679309	-0.059730	4.816006
292.479693	8000.137646	12.684314	-0.059758	4.816021
292.249891	8000.024447	12.689319	-0.059715	4.815990
292.151578	8000.076101	12.694323	-0.059697	4.816005
292.099760	7999.995007	12.699328	-0.059687	4.815982
292.085463	7999.972312	12.704333	-0.059685	4.815975
291.995006	8000.047621	12.709338	-0.059668	4.815998
292.065710	8000.028614	12.714343	-0.059681	4.815992
292.201037	8000.056741	12.719347	-0.059707	4.815999
291.850300	7999.952027	12.724352	-0.059641	4.815971
292.144088	7999.976632	12.729357	-0.059696	4.815976
292.368323	8000.067302	12.734362	-0.059738	4.816001
291.967364	7999.992664	12.739367	-0.059663	4.815982
292.358681	8000.048975	12.744371	-0.059736	4.815996
292.316141	8000.011869	12.749376	-0.059729	4.815985
292.416645	8000.086388	12.754381	-0.059747	4.816007
292.233036	8000.054191	12.759386	-0.059713	4.815998
292.285732	8000.038061	12.764391	-0.059723	4.815993
292.302433	8000.081125	12.769395	-0.059726	4.816006
292.232809	8000.049938	12.774400	-0.059714	4.815997
292.380965	8000.020587	12.779405	-0.059741	4.815988
292.233171	8000.085232	12.784410	-0.059714	4.816007
292.275107	8000.066768	12.789415	-0.059722	4.816002
292.344498	8000.101175	12.794419	-0.059735	4.816011
292.425295	7999.945549	12.799424	-0.059750	4.815966
292.317712	7999.988484	12.804429	-0.059730	4.815979
292.249472	7999.943429	12.809434	-0.059717	4.815966
292.139505	7999.971357	12.814439	-0.059697	4.815975
292.489204	8000.092104	12.819443	-0.059762	4.816008
292.324699	8000.035673	12.824448	-0.059732	4.815992
292.227202	8000.086273	12.829453	-0.059714	4.816008
292.253772	8000.041878	12.834458	-0.059719	4.815995
292.123817	8000.032035	12.839463	-0.059694	4.815992
292.097377	8000.065762	12.844467	-0.059690	4.816002
292.377725	7999.992865	12.849472	-0.059742	4.815980
292.297604	8000.019201	12.854477	-0.059727	4.815988
292.300526	8000.047051	12.859482	-0.059728	4.815996
292.361780	8000.025733	12.864487	-0.059739	4.815989
292.417088	8000.041714	12.869491	-0.059750	4.815994
292.175936	7999.960373	12.874496	-0.059705	4.815971
292.396388	8000.091586	12.879501	-0.059746	4.816008
292.343432	8000.073529	12.884506	-0.059736	4.816003
292.461492	7999.990190	12.889511	-0.059758	4.815978
292.424573	8000.083577	12.894515	-0.059752	4.816006
292.160491	8000.026399	12.899520	-0.059702	4.815990
292.400747	8000.083161	12.904525	-0.059747	4.816006
292.221438	8000.102342	12.909530	-0.059714	4.816012
292.208930	8000.025172	12.914535	-0.059712	4.815990
292.422365	8000.095338	12.919539	-0.059752	4.816009
292.276741	8000.093759	12.924544	-0.059725	4.816010
292.163005	7999.978404	12.929549	-0.059703	4.815976
292.154053	8000.060545	12.934554	-0.059702	4.816000
292.207003	8000.024113	12.939559	-0.059712	4.815990
292.160776	8000.097023	12.944563	-0.059703	4.816011
292.314789	8000.018616	12.949568	-0.059732	4.815987
292.267283	8000.015620	12.954573	-0.059723	4.815987
292.120225	8000.026841	12.959578	-0.059696	4.815991
292.245620	7999.966080	12.964583	-0.059719	4.815972
292.405730	8000.069474	12.969587	-0.059749	4.816002
292.346386	8000.057712	12.974592	-0.059738	4.815999
292.405893	8000.034225	12.979597	-0.059750	4.815991
292.276915	8000.067151	12.984602	-0.059726	4.816002
292.296105	8000.013003	12.989607	-0.059729	4.815986
292.246518	8000.073027	12.994611	-0.059720	4.816004
292.265611	8000.054146	12.999616	-0.059724	4.815998
292.365520	8000.051703	13.004621	-0.059743	4.815997
292.322269	8000.090467	13.009626	-0.059735	4.816008
292.402508	8000.101559	13.014631	-0.059750	4.816011
292.213439	8000.109875	13.019635	-0.059715	4.816015
292.011956	8000.079489	13.024640	-0.059677	4.816007
292.257141	8000.112828	13.029645	-0.059723	4.816015
292.429900	8000.097819	13.034650	-0.059755	4.816010
292.460867	8000.039611	13.039655	-0.059761	4.815993
292.372250	8000.105336	13.044659	-0.059745	4.816012
292.113576	7999.985199	13.049664	-0.059696	4.815979
292.317599	8000.064812	13.054669	-0.059735	4.816001
292.471949	8000.114663	13.059674	-0.059763	4.816015
292.325950	8000.025438	13.064679	-0.059736	4.815989
292.577153	8000.090950	13.069683	-0.059783	4.816007
292.500355	8000.058563	13.074688	-0.059769	4.815998
292.280231	8000.091963	13.079693	-0.059728	4.816009
292.375979	8000.095856	13.084698	-0.059746	4.816010
292.390922	8000.050181	13.089703	-0.059749	4.815996
292.341817	8000.054638	13.094707	-0.059740	4.815998
292.252714	8000.034852	13.099712	-0.059723	4.815992
292.493079	8000.075585	13.104717	-0.059768	4.816003
292.345108	8000.085719	13.109722	-0.059741	4.816007
292.265069	8000.021210	13.114727	-0.059726	4.815988
292.381864	8000.067170	13.119731	-0.059748	4.816001
292.343849	8000.077173	13.124736	-0.059741	4.816004
292.429915	8000.062720	13.129741	-0.059757	4.816000
292.674509	8000.085361	13.134746	-0.059802	4.816005
292.655830	8000.049760	13.139751	-0.059799	4.815995
292.403945	8000.153119	13.144755	-0.059752	4.816026
292.439833	8000.133476	13.149760	-0.059759	4.816020
292.485538	8000.093706	13.154765	-0.059768	4.816008
292.505563	8000.070567	13.159770	-0.059771	4.816001
292.235242	8000.059231	13.164775	-0.059721	4.816000
292.656203	8000.074402	13.169779	-0.059800	4.816002
292.600969	8000.056303	13.174784	-0.059789	4.815997
292.517928	8000.108236	13.179789	-0.059774	4.816012
292.191356	8000.060604	13.184794	-0.059713	4.816000
292.210344	8000.011796	13.189799	-0.059717	4.815986
292.433580	8000.133443	13.194803	-0.059759	4.816020
292.527378	8000.013323	13.199808	-0.059776	4.815985
292.603468	8000.072434	13.204813	-0.059790	4.816001
292.485358	8000.099145	13.209818	-0.059769	4.816010
292.368733	8000.068169	13.214823	-0.059747	4.816001
292.654003	8000.131097	13.219827	-0.059800	4.816018
292.404703	8000.116938	13.224832	-0.059754	4.816015
292.311106	8000.101345	13.229837	-0.059737	4.816011
292.498650	8000.150734	13.234842	-0.059772	4.816025
292.415995	8000.070145	13.239847	-0.059756	4.816002
292.557296	8000.120827	13.244851	-0.059783	4.816016
292.337913	8000.054844	13.249856	-0.059742	4.815998
292.459622	8000.074174	13.254861	-0.059765	4.816003
292.389833	8000.134899	13.259866	-0.059752	4.816021
292.424285	8000.061791	13.264871	-0.059758	4.815999
292.469589	8000.143853	13.269875	-0.059767	4.816023
292.476373	8000.078791	13.274880	-0.059768	4.816004
292.479063	8000.083124	13.279885	-0.059769	4.816005
292.399361	8000.131911	13.284890	-0.059754	4.816020
292.372082	8000.038439	13.289895	-0.059749	4.815993
292.634512	8000.099881	13.294899	-0.059798	4.816009
292.502046	8000.096404	13.299904	-0.059773	4.816009
292.406008	8000.074354	13.304909	-0.059756	4.816003
292.662783	8000.089736	13.309914	-0.059803	4.816006
292.278414	8000.080594	13.314919	-0.059732	4.816005
292.434800	8000.125139	13.319923	-0.059761	4.816018
292.604404	8000.098317	13.324928	-0.059793	4.816009
292.622277	8000.046282	13.329933	-0.059796	4.815994
292.590589	8000.097014	13.334938	-0.059790	4.816009
292.590585	8000.077785	13.339943	-0.059791	4.816003
292.495408	8000.146596	13.344947	-0.059773	4.816024
292.454712	8000.053948	13.349952	-0.059765	4.815997
292.635061	8000.063660	13.354957	-0.059799	4.815999
292.615420	8000.085755	13.359962	-0.059796	4.816005
292.374675	8000.022589	13.364967	-0.059751	4.815988
292.394004	8000.130897	13.369971	-0.059755	4.816020
292.538586	8000.052317	13.374976	-0.059782	4.815996
292.520050	8000.103289	13.379981	-0.059778	4.816011
292.419226	8000.168791	13.384986	-0.059760	4.816030
292.418854	8000.149555	13.389991	-0.059760	4.816025
292.607357	8000.164761	13.394995	-0.059795	4.816028
292.340368	8000.077602	13.400000	-0.059745	4.816004
292.498628	8000.095461	13.405005	-0.059775	4.816009
292.802385	8000.153384	13.410010	-0.059831	4.816024
292.469107	8000.113110	13.415015	-0.059769	4.816014
292.347486	8000.162201	13.420019	-0.059747	4.816029
292.421424	8000.080194	13.425024	-0.059761	4.816005
292.539761	8000.029992	13.430029	-0.059783	4.815989
292.581559	8000.118404	13.435034	-0.059791	4.816015
292.447697	8000.049706	13.440039	-0.059766	4.815995
292.515362	8000.127902	13.445043	-0.059779	4.816018
292.405174	8000.099181	13.450048	-0.059758	4.816010
292.391570	8000.110698	13.455053	-0.059756	4.816014
292.685413	7999.999572	13.460058	-0.059810	4.815980
292.598365	8000.006543	13.465063	-0.059794	4.815982
292.592343	8000.097288	13.470067	-0.059793	4.816009
292.657822	8000.096354	13.475072	-0.059806	4.816008
292.678644	8000.077505	13.480077	-0.059810	4.816002
292.704780	8000.142118	13.485082	-0.059815	4.816021
292.767288	8000.106929	13.490087	-0.059826	4.816010
292.994510	8000.152767	13.495091	-0.059869	4.816023
292.758627	8000.152746	13.500096	-0.059825	4.816024
292.802180	8000.114005	13.505101	-0.059833	4.816012
292.742851	8000.157820	13.510106	-0.059822	4.816025
292.572389	8000.059597	13.515111	-0.059790	4.815998
292.607836	8000.143618	13.520115	-0.059797	4.816022
292.520653	8000.121729	13.525120	-0.059781	4.816016
292.633941	8000.054334	13.530125	-0.059802	4.815996
292.509843	8000.137581	13.535130	-0.059779	4.816021
292.573889	8000.089595	13.540135	-0.059791	4.816006
292.853598	8000.147079	13.545139	-0.059843	4.816022
292.568132	8000.129053	13.550144	-0.059790	4.816018
292.732040	8000.112815	13.555149	-0.059821	4.816012
293.005540	8000.102852	13.560154	-0.059872	4.816008
292.652827	8000.098562	13.565159	-0.059806	4.816009
292.640058	8000.126126	13.570163	-0.059804	4.816017
292.736629	8000.096902	13.575168	-0.059822	4.816008
292.916932	8000.074551	13.580173	-0.059856	4.816000
292.724072	8000.140511	13.585178	-0.059820	4.816020
292.579698	8000.133611	13.590183	-0.059793	4.816019
292.891669	8000.090148	13.595187	-0.059851	4.816005
292.815522	8000.088768	13.600192	-0.059837	4.816005
292.866182	8000.145278	13.605197	-0.059847	4.816021
292.997337	8000.145543	13.610202	-0.059871	4.816020
292.813963	8000.075941	13.615207	-0.059837	4.816001
292.798798	8000.099186	13.620211	-0.059834	4.816008
292.690976	8000.105778	13.625216	-0.059814	4.816010
292.782487	8000.099975	13.630221	-0.059832	4.816008
292.820457	8000.144498	13.635226	-0.059839	4.816021
292.743561	8000.095008	13.640231	-0.059825	4.816007
292.893656	8000.110581	13.645235	-0.059853	4.816011
292.895130	8000.088173	13.650240	-0.059853	4.816004
292.790515	8000.046727	13.655245	-0.059834	4.815993
292.890027	8000.082753	13.660250	-0.059852	4.816003
292.666580	8000.017765	13.665255	-0.059811	4.815985
292.679184	8000.131294	13.670259	-0.059813	4.816018
292.734005	8000.106653	13.675264	-0.059823	4.816010
292.647784	8000.094401	13.680269	-0.059807	4.816007
292.824641	8000.128632	13.685274	-0.059840	4.816016
292.748381	7999.987239	13.690279	-0.059826	4.815976
292.739601	8000.080071	13.695283	-0.059825	4.816003
292.709347	8000.043190	13.700288	-0.059819	4.815992
292.668502	8000.053141	13.705293	-0.059812	4.815995
292.908155	8000.057523	13.710298	-0.059856	4.815995
292.942858	8000.025033	13.715303	-0.059863	4.815985
292.804954	8000.130473	13.720307	-0.059837	4.816017
292.899538	8000.092663	13.725312	-0.059855	4.816005
292.932328	8000.060138	13.730317	-0.059861	4.815996
292.918750	8000.071655	13.735322	-0.059859	4.815999
292.816309	8000.000324	13.740327	-0.059840	4.815979
292.882399	8000.019708	13.745331	-0.059852	4.815984
292.825970	8000.065714	13.750336	-0.059842	4.815998
292.767555	8000.013356	13.755341	-0.059831	4.815983
292.853243	8000.009584	13.760346	-0.059847	4.815981
292.839515	7999.959110	13.765351	-0.059845	4.815967
292.895662	8000.012514	13.770355	-0.059855	4.815982
292.975014	8000.007558	13.775360	-0.059870	4.815980
292.897131	7999.985839	13.780365	-0.059856	4.815974
292.937952	8000.061408	13.785370	-0.059863	4.815996
292.769907	8000.035906	13.790375	-0.059832	4.815990
293.108367	8000.104081	13.795379	-0.059895	4.816008
293.087405	8000.069506	13.800384	-0.059891	4.815998
292.885339	8000.018801	13.805389	-0.059854	4.815984
292.811905	8000.102972	13.810394	-0.059840	4.816009
292.915474	8000.027919	13.815399	-0.059860	4.815986
292.802663	8000.060070	13.820403	-0.059839	4.815996
292.738294	8000.092037	13.825408	-0.059827	4.816006
292.817830	8000.079603	13.830413	-0.059842	4.816002
292.916067	8000.158358	13.835418	-0.059860	4.816025
292.706638	8000.085073	13.840423	-0.059821	4.816004
292.795639	8000.115564	13.845427	-0.059838	4.816013
292.757556	8000.107396	13.850432	-0.059831	4.816010
292.822579	8000.042327	13.855437	-0.059843	4.815991
292.821287	8000.143847	13.860442	-0.059843	4.816021
292.731540	8000.083435	13.865447	-0.059826	4.816004
292.931109	8000.095636	13.870451	-0.059864	4.816006
292.830416	8000.056400	13.875456	-0.059845	4.815995
292.824450	8000.093708	13.880461	-0.059844	4.816006
292.805262	8000.143600	13.885466	-0.059841	4.816021
292.635952	8000.105249	13.890471	-0.059809	4.816010
292.814598	8000.114931	13.895475	-0.059842	4.816012
292.871316	8000.079636	13.900480	-0.059853	4.816002
292.771143	8000.056441	13.905485	-0.059834	4.815995
292.761304	8000.092609	13.910490	-0.059833	4.816006
292.947427	8000.076776	13.915495	-0.059868	4.816000
293.020844	8000.061025	13.920499	-0.059881	4.815995
292.878101	8000.104387	13.925504	-0.059855	4.816009
292.810521	8000.043310	13.930509	-0.059842	4.815991
292.963613	8000.093140	13.935514	-0.059871	4.816005
292.659836	8000.059817	13.940519	-0.059814	4.815997
292.932516	8000.089384	13.945523	-0.059865	4.816004
292.772547	8000.031965	13.950528	-0.059836	4.815988
292.829996	7999.982790	13.955533	-0.059846	4.815974
292.983931	8000.128825	13.960538	-0.059875	4.816015
292.834100	8000.116481	13.965543	-0.059847	4.816013
292.867073	8000.091440	13.970547	-0.059854	4.816005
292.872308	8000.117196	13.975552	-0.059855	4.816013
292.926467	8000.117124	13.980557	-0.059865	4.816012
293.131654	8000.201038	13.985562	-0.059903	4.816036
292.914460	8000.160744	13.990567	-0.059863	4.816025
292.732303	8000.110402	13.995571	-0.059829	4.816011
292.822995	8000.106722	14.000576	-0.059846	4.816010
292.867663	8000.123578	14.005581	-0.059854	4.816015
292.782186	8000.175466	14.010586	-0.059839	4.816030
292.710687	8000.088667	14.015591	-0.059825	4.816005
292.747998	8000.089357	14.020595	-0.059832	4.816005
292.685342	8000.148075	14.025600	-0.059821	4.816023
292.920936	8000.100012	14.030605	-0.059865	4.816007
293.009659	8000.149736	14.035610	-0.059881	4.816021
292.788918	8000.037769	14.040615	-0.059840	4.815990
292.905406	8000.111513	14.045619	-0.059862	4.816011
292.941314	8000.094007	14.050624	-0.059869	4.816005
292.910247	8000.034666	14.055629	-0.059863	4.815988
292.918484	8000.131016	14.060634	-0.059865	4.816016
292.989603	8000.083159	14.065639	-0.059878	4.816002
292.985602	8000.075613	14.070643	-0.059877	4.816000
292.819776	8000.074734	14.075648	-0.059847	4.816000
292.708106	8000.080186	14.080653	-0.059826	4.816003
292.931357	8000.167635	14.085658	-0.059868	4.816027
292.860120	8000.050915	14.090663	-0.059854	4.815993
293.039701	8000.077714	14.095667	-0.059888	4.816000
292.643742	8000.079048	14.100672	-0.059814	4.816003
292.850646	8000.046494	14.105677	-0.059853	4.815992
292.947551	8000.176526	14.110682	-0.059871	4.816030
292.970176	8000.076481	14.115687	-0.059875	4.816000
293.015020	8000.125404	14.120691	-0.059884	4.816014
292.826149	8000.121966	14.125696	-0.059849	4.816014
292.873040	8000.012746	14.130701	-0.059858	4.815982
292.883769	8000.078147	14.135706	-0.059860	4.816001
292.846689	8000.030452	14.140711	-0.059853	4.815987
292.892652	8000.089014	14.145715	-0.059862	4.816004
292.907991	8000.147018	14.150720	-0.059865	4.816021
292.813110	8000.146364	14.155725	-0.059847	4.816021
292.775124	8000.140336	14.160730	-0.059840	4.816020
292.769824	8000.069708	14.165735	-0.059839	4.815999
292.975246	8000.078810	14.170739	-0.059877	4.816001
292.792415	8000.138541	14.175744	-0.059843	4.816019
292.820100	8000.022557	14.180749	-0.059849	4.815985
292.774735	8000.111516	14.185754	-0.059840	4.816011
292.653313	8000.126410	14.190759	-0.059818	4.816016
292.578479	8000.131466	14.195763	-0.059804	4.816018
292.614487	8000.100069	14.200768	-0.059811	4.816009
292.712870	8000.084772	14.205773	-0.059829	4.816004
292.706597	8000.112455	14.210778	-0.059828	4.816012
292.685456	8000.061846	14.215783	-0.059824	4.815997
293.032523	8000.028643	14.220787	-0.059889	4.815986
292.945868	8000.065547	14.225792	-0.059873	4.815997
292.677591	8000.091655	14.230797	-0.059823	4.816006
292.773575	8000.117998	14.235802	-0.059841	4.816013
292.673216	7999.084829	14.240807	-0.059822	4.815712

292.804435	7995.990365	14.245811	-0.059844	4.814807
292.728806	7990.578914	14.250816	-0.059827	4.813226
292.852693	7983.935278	14.255821	-0.059846	4.811283
292.696236	7976.631888	14.260826	-0.059812	4.809148
292.325366	7968.978154	14.265831	-0.059738	4.806911
292.487941	7961.176352	14.270835	-0.059763	4.804626
292.417330	7953.380615	14.275840	-0.059745	4.802343
292.353352	7945.336274	14.280845	-0.059728	4.799986
292.530883	7937.483081	14.285850	-0.059756	4.797683
292.423487	7929.380939	14.290855	-0.059731	4.795308
292.430107	7921.391088	14.295859	-0.059727	4.792963
292.407249	7913.387667	14.300864	-0.059717	4.790613
292.401237	7905.451152	14.305869	-0.059711	4.788282
292.199042	7897.330623	14.310874	-0.059668	4.785897
291.997487	7889.341626	14.315879	-0.059626	4.783549
292.292731	7881.389726	14.320883	-0.059676	4.781208
292.282357	7873.434863	14.325888	-0.059669	4.778867
292.260998	7865.429687	14.330893	-0.059660	4.776510
292.263778	7857.421420	14.335898	-0.059655	4.774150
291.996650	7849.357064	14.340903	-0.059600	4.771775
292.052513	7841.407318	14.345907	-0.059605	4.769430
291.887239	7833.396976	14.350912	-0.059569	4.767067
292.018357	7825.360986	14.355917	-0.059589	4.764694
291.981937	7817.467206	14.360922	-0.059577	4.762363
291.739588	7809.329452	14.365927	-0.059527	4.759960
291.765833	7801.428610	14.370931	-0.059526	4.757624
291.666841	7793.350601	14.375936	-0.059503	4.755235
291.522929	7785.337288	14.380941	-0.059471	4.752864
291.514192	7777.356123	14.385946	-0.059464	4.750501
291.446745	7769.322357	14.390951	-0.059446	4.748121
291.415927	7761.362613	14.395955	-0.059436	4.745762
291.413224	7753.356667	14.400960	-0.059430	4.743388
291.341812	7745.318142	14.405965	-0.059411	4.741004
291.353114	7737.375108	14.410970	-0.059409	4.738646
291.226717	7729.305155	14.415975	-0.059380	4.736250
291.347779	7721.350372	14.420979	-0.059397	4.733886
291.242764	7713.286739	14.425984	-0.059373	4.731489
291.128211	7705.305842	14.430989	-0.059346	4.729116
291.125833	7697.349100	14.435994	-0.059341	4.726748
291.126331	7689.289454	14.440999	-0.059335	4.724348
291.104397	7681.336362	14.446003	-0.059326	4.721979
290.947141	7673.310484	14.451008	-0.059292	4.719588
290.933043	7665.341476	14.456013	-0.059284	4.717212
290.979596	7657.312230	14.461018	-0.059288	4.714816
290.752812	7649.278136	14.466023	-0.059240	4.712419
291.055091	7641.300276	14.471027	-0.059291	4.710036
291.017893	7633.336773	14.476032	-0.059279	4.707656
290.665560	7625.252293	14.481037	-0.059209	4.705241
290.709939	7617.342609	14.486042	-0.059212	4.702875
290.595032	7609.283229	14.491047	-0.059185	4.700463
290.521500	7601.363912	14.496051	-0.059167	4.698092
290.546957	7593.321292	14.501056	-0.059166	4.695683
290.350626	7585.314324	14.506061	-0.059124	4.693284
290.511816	7577.257117	14.511066	-0.059149	4.690867
290.393472	7569.266351	14.516071	-0.059122	4.688470
290.298656	7561.290301	14.521075	-0.059099	4.686076
290.370635	7553.301927	14.526080	-0.059108	4.683677
290.267643	7545.303913	14.531085	-0.059083	4.681274
290.150309	7537.369132	14.536090	-0.059056	4.678889
290.199422	7529.304677	14.541095	-0.059060	4.676463
290.125897	7521.218701	14.546099	-0.059042	4.674030
290.103778	7513.161142	14.551104	-0.059032	4.671604
289.948952	7505.197104	14.556109	-0.058998	4.669205
289.903096	7497.259623	14.561114	-0.058985	4.666812
289.729856	7489.227181	14.566119	-0.058947	4.664390
289.805682	7481.232442	14.571123	-0.058956	4.661978
290.012659	7473.237356	14.576128	-0.058990	4.659564
289.794408	7465.250338	14.581133	-0.058944	4.657152
289.687136	7457.270170	14.586138	-0.058919	4.654741
289.707058	7449.229762	14.591143	-0.058918	4.652310
289.761739	7441.176179	14.596147	-0.058923	4.649873
289.760462	7433.279176	14.601152	-0.058917	4.647483
289.829472	7425.188650	14.606157	-0.058925	4.645033
289.771904	7417.296562	14.611162	-0.058909	4.642642
289.610942	7409.221819	14.616167	-0.058874	4.640194
289.610957	7401.247692	14.621171	-0.058869	4.637775
289.425526	7393.187617	14.626176	-0.058829	4.635330
289.525842	7385.164667	14.631181	-0.058843	4.632893
289.422953	7377.182277	14.636186	-0.058818	4.630469
289.380845	7369.214558	14.641191	-0.058806	4.628047
289.430139	7361.157879	14.646195	-0.058810	4.625597
289.170368	7353.229848	14.651200	-0.058756	4.623185
289.039502	7345.186400	14.656205	-0.058727	4.620736
289.159683	7337.244113	14.661210	-0.058744	4.618317
289.048546	7329.170329	14.666215	-0.058718	4.615856
288.965963	7321.179768	14.671219	-0.058698	4.613420
289.091869	7313.150806	14.676224	-0.058716	4.610970
288.864055	7305.194129	14.681229	-0.058668	4.608542
288.967790	7297.189979	14.686234	-0.058683	4.606097
288.909319	7289.188881	14.691239	-0.058667	4.603652
288.785901	7281.196104	14.696243	-0.058638	4.601209
288.769875	7273.224008	14.701248	-0.058630	4.598770
288.810702	7265.176627	14.706253	-0.058633	4.596307
288.903068	7257.157000	14.711258	-0.058645	4.593852
288.622416	7249.086658	14.716263	-0.058587	4.591379
288.707135	7241.088893	14.721267	-0.058598	4.588927
288.691339	7233.148342	14.726272	-0.058590	4.586492
288.636402	7225.140855	14.731277	-0.058575	4.584034
288.478703	7217.196739	14.736282	-0.058540	4.581595
288.464185	7209.130790	14.741287	-0.058532	4.579117
288.488526	7201.167668	14.746291	-0.058532	4.576670
288.378459	7193.139989	14.751296	-0.058506	4.574201
288.271908	7185.081188	14.756301	-0.058481	4.571721
288.192229	7177.113945	14.761306	-0.058461	4.569268
288.143914	7169.108400	14.766311	-0.058447	4.566802
288.207042	7161.141387	14.771315	-0.058454	4.564346
288.344104	7153.188587	14.776320	-0.058474	4.561894
288.123488	7145.106418	14.781325	-0.058428	4.559400
288.083059	7137.182944	14.786330	-0.058415	4.556954
287.863162	7129.082405	14.791335	-0.058369	4.554452
288.037797	7121.076034	14.796339	-0.058397	4.551978
287.963174	7113.109127	14.801344	-0.058378	4.549514
287.809587	7105.105495	14.806349	-0.058344	4.547038
287.784741	7097.115885	14.811354	-0.058334	4.544565
287.755693	7089.151822	14.816359	-0.058324	4.542098
287.745147	7081.133610	14.821363	-0.058317	4.539613
287.705933	7073.177305	14.826368	-0.058304	4.537146
287.755059	7065.094156	14.831373	-0.058308	4.534638
287.662399	7057.130774	14.836378	-0.058286	4.532166
287.543063	7049.049309	14.841383	-0.058258	4.529656
287.601006	7041.134174	14.846387	-0.058264	4.527197
287.537684	7033.119577	14.851392	-0.058247	4.524705
287.351241	7025.154258	14.856397	-0.058207	4.522227
287.439714	7017.131639	14.861402	-0.058219	4.519730
287.270381	7009.158056	14.866407	-0.058182	4.517246
287.308438	7001.078480	14.871411	-0.058184	4.514728
287.369006	6993.064327	14.876416	-0.058190	4.512230
287.175234	6985.037251	14.881421	-0.058149	4.509725
287.218234	6977.065121	14.886426	-0.058152	4.507237
287.186181	6969.038940	14.891431	-0.058141	4.504731
287.205114	6961.093795	14.896435	-0.058139	4.502248
287.084432	6953.090165	14.901440	-0.058112	4.499745
286.743044	6945.059778	14.906445	-0.058043	4.497232
286.754462	6937.091131	14.911450	-0.058040	4.494738
286.913970	6929.057969	14.916455	-0.058064	4.492223
286.745411	6921.072750	14.921459	-0.058028	4.489720
286.666865	6913.096287	14.926464	-0.058008	4.487219
286.693112	6905.052781	14.931469	-0.058008	4.484696
286.647357	6897.093974	14.936474	-0.057994	4.482198
286.449033	6889.042600	14.941479	-0.057952	4.479669
286.576514	6881.095204	14.946483	-0.057971	4.477172
286.611871	6873.098456	14.951488	-0.057972	4.474658
286.520476	6865.013145	14.956493	-0.057950	4.472114
286.698027	6857.056799	14.961498	-0.057978	4.469610
286.568915	6849.021657	14.966503	-0.057949	4.467079
286.384932	6841.019412	14.971507	-0.057910	4.464557
286.283117	6833.074381	14.976512	-0.057885	4.462051
286.201967	6825.018884	14.981517	-0.057865	4.459510
286.276652	6817.058315	14.986522	-0.057874	4.456997
286.164973	6809.027154	14.991527	-0.057848	4.454460
286.298880	6800.988034	14.996531	-0.057868	4.451920
286.086656	6793.053091	15.001536	-0.057823	4.449410
285.843127	6784.997789	15.006541	-0.057773	4.446861
285.877089	6777.017931	15.011546	-0.057774	4.444335
285.945991	6769.025440	15.016551	-0.057782	4.441803
286.028417	6761.031414	15.021555	-0.057792	4.439270
285.821878	6753.059234	15.026560	-0.057748	4.436741
285.759697	6744.995466	15.031565	-0.057732	4.434183
285.812749	6736.973274	15.036570	-0.057736	4.431636
285.559242	6728.946831	15.041575	-0.057684	4.429085
285.604927	6720.963458	15.046579	-0.057687	4.426548
285.735152	6713.017887	15.051584	-0.057707	4.424022
285.605477	6705.053805	15.056589	-0.057677	4.421487
285.475366	6697.049263	15.061594	-0.057648	4.418938
285.455733	6688.962644	15.066599	-0.057639	4.416362
285.318991	6680.966601	15.071603	-0.057609	4.413812
285.160492	6672.958913	15.076608	-0.057574	4.411257
285.247033	6664.971976	15.081613	-0.057585	4.408709
284.999815	6656.982760	15.086618	-0.057534	4.406157
284.873148	6648.952543	15.091623	-0.057505	4.403590
284.977643	6640.948017	15.096627	-0.057519	4.401032
285.329619	6633.030229	15.101632	-0.057580	4.398501
285.018049	6625.006122	15.106637	-0.057517	4.395931
285.110875	6617.019543	15.111642	-0.057529	4.393374
284.951887	6608.964597	15.116647	-0.057494	4.390792
285.007158	6600.982111	15.121651	-0.057499	4.388233
284.989556	6592.958744	15.126656	-0.057491	4.385659
284.634680	6584.979635	15.131661	-0.057420	4.383096
284.779713	6577.017497	15.136666	-0.057442	4.380539
284.737822	6569.002867	15.141671	-0.057429	4.377963
284.630582	6560.983408	15.146675	-0.057404	4.375384
284.542386	6553.024663	15.151680	-0.057382	4.372822
284.362667	6544.964600	15.156685	-0.057343	4.370227
284.366257	6537.024401	15.161690	-0.057339	4.367669
284.307516	6528.936006	15.166695	-0.057323	4.365061
284.422045	6521.043885	15.171699	-0.057339	4.362516
284.294149	6513.020477	15.176704	-0.057310	4.359926
284.150848	6505.019576	15.181709	-0.057278	4.357342
284.377762	6496.964489	15.186714	-0.057315	4.354741
284.040362	6488.894735	15.191719	-0.057247	4.352130
284.000884	6480.909253	15.196723	-0.057235	4.349546
284.039388	6472.941518	15.201728	-0.057237	4.346968
284.070198	6464.896739	15.206733	-0.057238	4.344362
283.967459	6457.013472	15.211738	-0.057214	4.341807
283.852435	6448.972471	15.216743	-0.057187	4.339199
283.922415	6440.949042	15.221747	-0.057195	4.336596
283.783204	6432.954789	15.226752	-0.057164	4.334000
283.710674	6424.936178	15.231757	-0.057145	4.331394
283.815057	6416.963946	15.236762	-0.057159	4.328804
283.730054	6408.961012	15.241767	-0.057139	4.326200
283.746449	6400.962746	15.246771	-0.057136	4.323598
283.672098	6392.985580	15.251776	-0.057118	4.320999
283.500017	6384.996163	15.256781	-0.057080	4.318395
283.357295	6376.979425	15.261786	-0.057049	4.315780
283.288876	6368.894254	15.266791	-0.057031	4.313142
283.406583	6360.895104	15.271795	-0.057048	4.310532
283.367691	6352.936692	15.276800	-0.057035	4.307932
283.323321	6344.911605	15.281805	-0.057022	4.305309
283.413692	6336.982905	15.286810	-0.057034	4.302717
283.144428	6328.944983	15.291815	-0.056978	4.300085
283.187823	6320.949784	15.296819	-0.056981	4.297467
283.259582	6312.949268	15.301824	-0.056989	4.294847
283.205221	6304.919405	15.306829	-0.056974	4.292214
283.121415	6296.918972	15.311834	-0.056953	4.289589
283.017944	6288.930597	15.316839	-0.056929	4.286966
282.979502	6280.940866	15.321843	-0.056917	4.284342
283.003769	6272.983993	15.326848	-0.056916	4.281727
283.055888	6264.928801	15.331853	-0.056921	4.279079
283.050311	6256.972943	15.336858	-0.056915	4.276461
282.934746	6248.891949	15.341863	-0.056888	4.273799
282.737848	6240.867317	15.346867	-0.056846	4.271154
282.694462	6232.897886	15.351872	-0.056833	4.268527
282.581892	6224.866999	15.356877	-0.056807	4.265877
282.792512	6216.916191	15.361882	-0.056841	4.263254
282.704710	6208.874800	15.366887	-0.056820	4.260598
282.652191	6200.969780	15.371891	-0.056805	4.257985
282.640870	6192.926055	15.376896	-0.056797	4.255325
282.630319	6184.931684	15.381901	-0.056790	4.252680
282.547573	6176.898006	15.386906	-0.056770	4.250019
282.547234	6168.950120	15.391911	-0.056765	4.247386
282.490673	6160.890044	15.396915	-0.056749	4.244714
282.494091	6152.976478	15.401920	-0.056745	4.242089
282.250821	6144.929685	15.406925	-0.056694	4.239416
282.186797	6137.003471	15.411930	-0.056677	4.236782
282.037343	6128.896740	15.416935	-0.056644	4.234087
282.274228	6120.874657	15.421939	-0.056683	4.231421
282.234050	6112.909337	15.426944	-0.056670	4.228770
282.095034	6104.911500	15.431949	-0.056639	4.226106
282.019093	6096.939473	15.436954	-0.056620	4.223449
281.980251	6088.951787	15.441959	-0.056608	4.220786
281.912344	6080.944738	15.446963	-0.056590	4.218114
282.043436	6072.968852	15.451968	-0.056609	4.215453
281.776084	6064.968404	15.456973	-0.056554	4.212778
281.872387	6056.924248	15.461978	-0.056567	4.210090
281.690936	6048.977350	15.466983	-0.056528	4.207431
281.554822	6040.891533	15.471987	-0.056498	4.204723
281.692287	6032.988299	15.476992	-0.056518	4.202078
281.454062	6024.944786	15.481997	-0.056469	4.199380
281.472600	6016.977914	15.487002	-0.056467	4.196709
281.426057	6008.885075	15.492007	-0.056453	4.193993
281.270663	6000.821284	15.497011	-0.056419	4.191284
281.430149	5992.884074	15.502016	-0.056444	4.188619
281.504739	5984.868147	15.507021	-0.056453	4.185925
281.452586	5976.948518	15.512026	-0.056438	4.183261
281.214645	5968.928527	15.517031	-0.056388	4.180559
281.241499	5960.936049	15.522035	-0.056388	4.177867
281.212031	5952.949580	15.527040	-0.056378	4.175175
281.052683	5944.907654	15.532045	-0.056343	4.172461
281.207987	5936.915484	15.537050	-0.056367	4.169765
281.208897	5928.925099	15.542055	-0.056362	4.167067
281.010187	5920.856803	15.547059	-0.056320	4.164338
280.965051	5912.960533	15.552064	-0.056306	4.161668
280.815514	5904.915066	15.557069	-0.056273	4.158944
280.837283	5896.945775	15.562074	-0.056272	4.156246
280.672668	5888.896669	15.567079	-0.056236	4.153517
280.566432	5880.874907	15.572083	-0.056211	4.150796
280.736011	5872.868480	15.577088	-0.056238	4.148082
280.545518	5864.877597	15.582093	-0.056197	4.145367
280.710220	5856.946995	15.587098	-0.056223	4.142675
280.553553	5848.872749	15.592103	-0.056188	4.139928
280.341349	5840.909529	15.597107	-0.056144	4.137217
280.475222	5832.872687	15.602112	-0.056164	4.134483
280.693784	5824.868399	15.607117	-0.056199	4.131760
280.637099	5816.866138	15.612122	-0.056184	4.129032
280.224971	5808.911928	15.617127	-0.056102	4.126314
280.347643	5800.931371	15.622131	-0.056119	4.123592
280.488291	5792.919757	15.627136	-0.056140	4.120858
280.486277	5784.941357	15.632141	-0.056135	4.118131
280.279245	5776.922701	15.637146	-0.056091	4.115387
280.276784	5768.870153	15.642151	-0.056086	4.112631
280.244921	5760.849602	15.647155	-0.056075	4.109884
279.980371	5752.909448	15.652160	-0.056020	4.107160
279.934158	5744.902012	15.657165	-0.056007	4.104414
280.146497	5736.924046	15.662170	-0.056041	4.101680
279.824120	5728.941221	15.667175	-0.055976	4.098935
279.809045	5720.899701	15.672179	-0.055968	4.096172
279.900581	5712.907725	15.677184	-0.055980	4.093425
279.761858	5704.886240	15.682189	-0.055949	4.090664
279.880642	5696.961082	15.687194	-0.055966	4.087937
279.944549	5688.913713	15.692199	-0.055973	4.085166
279.832656	5680.943719	15.697203	-0.055947	4.082417
279.699644	5672.937439	15.702208	-0.055917	4.079653
279.725448	5664.960324	15.707213	-0.055917	4.076900
279.638483	5656.956849	15.712218	-0.055895	4.074134
279.523034	5648.917533	15.717223	-0.055869	4.071354
279.565978	5640.916327	15.722227	-0.055871	4.068587
279.519152	5632.926810	15.727232	-0.055858	4.065821
279.320152	5624.948805	15.732237	-0.055815	4.063055
279.203775	5616.957717	15.737242	-0.055789	4.060283
279.149355	5608.989448	15.742247	-0.055773	4.057519
279.085266	5600.924524	15.747251	-0.055756	4.054719
279.106069	5592.931851	15.752256	-0.055755	4.051943
278.972626	5584.921304	15.757261	-0.055725	4.049157
279.092141	5576.944566	15.762266	-0.055742	4.046384
279.126820	5568.999158	15.767271	-0.055744	4.043619
278.874061	5560.946497	15.772275	-0.055691	4.040811
279.055092	5552.998846	15.777280	-0.055720	4.038044
278.838149	5544.945209	15.782285	-0.055674	4.035232
278.969961	5536.853162	15.787290	-0.055694	4.032409
279.039839	5528.873889	15.792295	-0.055702	4.029624
278.795494	5520.894649	15.797299	-0.055651	4.026831
278.613142	5512.913065	15.802304	-0.055612	4.024037
278.517823	5504.908426	15.807309	-0.055589	4.021234
278.577957	5496.966017	15.812314	-0.055595	4.018453
278.505829	5488.944847	15.817319	-0.055577	4.015641
278.348765	5480.924109	15.822323	-0.055542	4.012826
278.473594	5472.948397	15.827328	-0.055560	4.010028
278.528792	5464.964361	15.832333	-0.055566	4.007225
278.191082	5456.901009	15.837338	-0.055498	4.004386
278.190489	5448.973313	15.842343	-0.055492	4.001598
278.222692	5440.934424	15.847347	-0.055493	3.998769
278.392860	5432.939391	15.852352	-0.055520	3.995956
278.095804	5424.892856	15.857357	-0.055459	3.993115
278.226666	5416.885202	15.862362	-0.055479	3.990293
278.287834	5408.924325	15.867367	-0.055485	3.987484
278.047745	5400.904021	15.872371	-0.055435	3.984647
278.105271	5392.988157	15.877376	-0.055441	3.981850
278.009522	5384.941890	15.882381	-0.055418	3.979002
277.940082	5376.961063	15.887386	-0.055400	3.976176
277.757079	5368.970905	15.892391	-0.055360	3.973343
277.736557	5360.928840	15.897395	-0.055352	3.970492
277.569187	5352.955687	15.902400	-0.055315	3.967661
277.448399	5344.914920	15.907405	-0.055288	3.964805
277.656507	5336.985856	15.912410	-0.055321	3.961992
277.560433	5328.994987	15.917415	-0.055298	3.959149
277.435907	5321.004228	15.922419	-0.055270	3.956305
277.455263	5312.990545	15.927424	-0.055268	3.953452
277.330741	5304.961456	15.932429	-0.055240	3.950589
277.345055	5296.973632	15.937434	-0.055238	3.947742
277.254131	5288.933640	15.942439	-0.055216	3.944872
277.259267	5280.985824	15.947443	-0.055211	3.942034
277.248588	5272.998207	15.952448	-0.055204	3.939180
277.196626	5264.993955	15.957453	-0.055190	3.936317
277.128143	5256.986766	15.962458	-0.055172	3.933451
277.176432	5248.977993	15.967463	-0.055176	3.930584
276.942949	5240.994117	15.972467	-0.055127	3.927719
276.862892	5232.992941	15.977472	-0.055107	3.924848
276.743304	5224.990921	15.982477	-0.055080	3.921974
276.634405	5217.026445	15.987482	-0.055054	3.919112
276.650817	5209.045957	15.992487	-0.055052	3.916244
276.812443	5200.991151	15.997491	-0.055077	3.913350
276.873224	5192.983730	16.002496	-0.055083	3.910469
276.574224	5185.013354	16.007501	-0.055022	3.907593
276.583887	5177.007362	16.012506	-0.055019	3.904707
276.658613	5169.035125	16.017511	-0.055028	3.901833
276.554489	5161.008713	16.022515	-0.055003	3.898933
276.398948	5153.016874	16.027520	-0.054969	3.896043
276.335463	5144.981414	16.032525	-0.054952	3.893137
276.331512	5136.987728	16.037530	-0.054947	3.890245
276.256574	5129.020915	16.042535	-0.054927	3.887359
276.336353	5120.982239	16.047539	-0.054937	3.884448
276.404271	5113.068951	16.052544	-0.054945	3.881579
276.120344	5105.058680	16.057549	-0.054887	3.878667
276.101965	5097.032842	16.062554	-0.054878	3.875752
276.080182	5088.826900	16.067559	-0.054869	3.872769
275.809759	5080.776052	16.072563	-0.054813	3.869836
275.949012	5072.900822	16.077568	-0.054834	3.866972
275.872013	5064.909272	16.082573	-0.054815	3.864060
275.853912	5056.976276	16.087578	-0.054806	3.861167
275.867985	5049.020132	16.092583	-0.054804	3.858265
275.850383	5040.981931	16.097587	-0.054795	3.855330
276.058613	5033.017915	16.102592	-0.054829	3.852425
275.922416	5024.993209	16.107597	-0.054799	3.849488
275.952975	5017.012496	16.112602	-0.054799	3.846568
275.822566	5009.018532	16.117607	-0.054770	3.843638
275.681875	5001.027885	16.122611	-0.054739	3.840707
275.769093	4993.079333	16.127616	-0.054750	3.837793
275.742319	4985.041916	16.132621	-0.054740	3.834843
275.728046	4977.055888	16.137626	-0.054732	3.831909
275.531456	4969.047951	16.142631	-0.054690	3.828961
275.569054	4961.017051	16.147635	-0.054692	3.826007
275.319046	4953.091561	16.152640	-0.054640	3.823084
275.166370	4945.066819	16.157645	-0.054607	3.820124
275.265779	4937.093359	16.162650	-0.054620	3.817186
275.351333	4929.111565	16.167655	-0.054631	3.814242
275.412656	4921.068836	16.172659	-0.054637	3.811273
275.253764	4913.091373	16.177664	-0.054602	3.808322
274.873067	4905.094075	16.182669	-0.054526	3.805355
274.826035	4897.118558	16.187674	-0.054513	3.802402
274.959961	4889.126185	16.192679	-0.054532	3.799444
275.141706	4881.086713	16.197683	-0.054561	3.796467
275.113596	4873.094262	16.202688	-0.054551	3.793501
274.700729	4865.081769	16.207693	-0.054469	3.790517
274.681702	4857.098921	16.212698	-0.054460	3.787549
274.745248	4849.087290	16.217703	-0.054467	3.784571
274.681993	4841.091088	16.222707	-0.054450	3.781593
274.724275	4833.106712	16.227712	-0.054453	3.778620
274.763290	4825.097831	16.232717	-0.054455	3.775635
274.486644	4817.110698	16.237722	-0.054398	3.772649
274.301520	4809.097812	16.242727	-0.054359	3.769652
274.389655	4801.104255	16.247731	-0.054370	3.766667
274.608785	4793.102460	16.252736	-0.054406	3.763679
274.219495	4785.150257	16.257741	-0.054328	3.760694
274.403310	4777.155741	16.262746	-0.054357	3.757704
274.452220	4769.134075	16.267751	-0.054361	3.754697
274.240452	4761.106396	16.272755	-0.054317	3.751681
274.209229	4753.112484	16.277760	-0.054306	3.748678
274.006357	4745.103121	16.282765	-0.054263	3.745664
274.017010	4737.136141	16.287770	-0.054260	3.742667
273.965099	4729.139601	16.292775	-0.054245	3.739656
273.794203	4721.178424	16.297779	-0.054208	3.736653
273.938431	4713.147075	16.302784	-0.054230	3.733629
273.620871	4705.135186	16.307789	-0.054165	3.730598
273.579494	4697.182964	16.312794	-0.054153	3.727594
273.720127	4689.138258	16.317799	-0.054174	3.724557
273.541750	4681.181141	16.322803	-0.054135	3.721543
273.656036	4673.193986	16.327808	-0.054151	3.718522
273.725264	4665.183175	16.332813	-0.054159	3.715489
273.443760	4657.131974	16.337818	-0.054102	3.712429
273.451860	4649.145610	16.342823	-0.054098	3.709399
273.354997	4641.133028	16.347827	-0.054075	3.706353
273.722269	4633.163897	16.352832	-0.054138	3.703333
273.566981	4625.189515	16.357837	-0.054104	3.700296
273.330491	4617.249112	16.362842	-0.054055	3.697267
273.347697	4609.221149	16.367847	-0.054053	3.694208
273.201704	4601.173576	16.372851	-0.054021	3.691135
273.167810	4593.231785	16.377856	-0.054009	3.688103
273.100859	4585.221090	16.382861	-0.053992	3.685042
273.173684	4577.252852	16.387866	-0.054000	3.681997
273.129003	4569.241787	16.392871	-0.053987	3.678931
272.980603	4561.253206	16.397875	-0.053954	3.675868
273.108148	4553.242584	16.402880	-0.053973	3.672800
272.857871	4545.236731	16.407885	-0.053921	3.669723
272.903602	4537.240033	16.412890	-0.053924	3.666654
273.006476	4529.242155	16.417895	-0.053938	3.663584
272.985340	4521.233245	16.422899	-0.053929	3.660503
272.836812	4513.303666	16.427904	-0.053896	3.657447
272.771721	4505.248000	16.432909	-0.053879	3.654343
272.686850	4497.252350	16.437914	-0.053858	3.651258
272.632211	4489.301898	16.442919	-0.053843	3.648188
272.640726	4481.249654	16.447923	-0.053839	3.645079
272.704238	4473.322464	16.452928	-0.053846	3.642017
272.627954	4465.291237	16.457933	-0.053827	3.638908
272.534599	4457.301929	16.462938	-0.053804	3.635812
272.392046	4449.281770	16.467943	-0.053773	3.632700
272.203356	4441.254824	16.472947	-0.053732	3.629582
272.113085	4433.312503	16.477952	-0.053711	3.626496
272.140779	4425.282095	16.482957	-0.053711	3.623377
272.300397	4417.262304	16.487962	-0.053735	3.620263
272.038120	4409.331557	16.492967	-0.053681	3.617169
272.037458	4401.281350	16.497971	-0.053676	3.614034
272.085064	4393.295601	16.502976	-0.053680	3.610922
272.100212	4385.316594	16.507981	-0.053677	3.607809
271.928980	4377.316804	16.512986	-0.053640	3.604680
271.996406	4369.416619	16.517991	-0.053648	3.601594
271.747014	4361.397175	16.522995	-0.053596	3.598450
271.801910	4353.372086	16.528000	-0.053601	3.595309
271.493525	4345.373405	16.533005	-0.053539	3.592166
271.752775	4337.361359	16.538010	-0.053582	3.589030
271.807959	4329.365998	16.543015	-0.053587	3.585893
271.522222	4321.401219	16.548019	-0.053529	3.582755
271.493608	4313.417958	16.553024	-0.053518	3.579615
271.642761	4305.424175	16.558029	-0.053541	3.576473
271.576955	4297.400585	16.563034	-0.053524	3.573310
271.401436	4289.420562	16.568039	-0.053486	3.570158
271.173640	4281.443556	16.573043	-0.053438	3.567003
271.227504	4273.458759	16.578048	-0.053443	3.563851
271.293012	4265.447799	16.583053	-0.053450	3.560685
271.322531	4257.457611	16.588058	-0.053451	3.557524
271.261102	4249.441002	16.593063	-0.053434	3.554347
270.887814	4241.340382	16.598067	-0.053359	3.551125
271.001498	4233.382841	16.603072	-0.053376	3.547971
270.974886	4225.396340	16.608077	-0.053365	3.544798
270.900968	4217.452699	16.613082	-0.053347	3.541639
270.786145	4209.481576	16.618087	-0.053320	3.538464
270.721853	4201.459830	16.623091	-0.053303	3.535267
270.932735	4193.449092	16.628096	-0.053337	3.532081
270.814512	4185.461531	16.633101	-0.053310	3.528891
270.810177	4177.435191	16.638106	-0.053304	3.525686
270.823796	4169.488980	16.643111	-0.053302	3.522510
270.426447	4161.526341	16.648115	-0.053222	3.519313
270.728998	4153.545449	16.653120	-0.053274	3.516127
270.550007	4145.509294	16.658125	-0.053235	3.512901
270.390637	4137.473671	16.663130	-0.053200	3.509673
270.293384	4129.520061	16.668135	-0.053177	3.506476
270.334023	4121.496432	16.673139	-0.053180	3.503253
270.316800	4113.552103	16.678144	-0.053171	3.500057
270.175145	4105.574997	16.683149	-0.053140	3.496841
270.245653	4097.550239	16.688154	-0.053148	3.493610
270.388495	4089.562882	16.693159	-0.053169	3.490392
270.050120	4081.569840	16.698163	-0.053101	3.487155
269.963834	4073.604201	16.703168	-0.053080	3.483933
269.862414	4065.636352	16.708173	-0.053056	3.480707
269.738301	4057.632235	16.713178	-0.053028	3.477463
269.647186	4049.639230	16.718183	-0.053006	3.474221
269.575232	4041.568373	16.723187	-0.052987	3.470945
269.777378	4033.583553	16.728192	-0.053020	3.467710
269.537721	4025.604811	16.733197	-0.052970	3.464460
269.610300	4017.609780	16.738202	-0.052978	3.461210
269.653460	4009.659049	16.743207	-0.052981	3.457975
269.336020	4001.650178	16.748211	-0.052917	3.454700
269.357000	3993.651963	16.753216	-0.052916	3.451439
269.334701	3985.660934	16.758221	-0.052907	3.448175
269.331330	3977.628631	16.763226	-0.052901	3.444892
269.327538	3969.709296	16.768231	-0.052895	3.441653
269.357128	3961.638510	16.773235	-0.052895	3.438349
269.579470	3953.684814	16.778240	-0.052932	3.435096
269.242838	3945.672624	16.783245	-0.052864	3.431798
269.049657	3937.686326	16.788250	-0.052823	3.428512
269.102393	3929.671888	16.793255	-0.052827	3.425220
269.138409	3921.718828	16.798259	-0.052829	3.421949
269.066692	3913.737436	16.803264	-0.052811	3.418660
269.039993	3905.723750	16.808269	-0.052801	3.415355
269.044382	3897.727392	16.813274	-0.052796	3.412056
268.809003	3889.753920	16.818279	-0.052747	3.408755
268.771292	3881.727490	16.823283	-0.052735	3.405435
268.897919	3873.791871	16.828288	-0.052754	3.402156
268.745613	3865.804047	16.833293	-0.052720	3.398842
268.848223	3857.784148	16.838298	-0.052734	3.395520
268.903590	3849.714328	16.843303	-0.052739	3.392172
268.697628	3841.704256	16.848307	-0.052696	3.388837
268.563322	3833.760720	16.853312	-0.052666	3.385529
268.568748	3825.797584	16.858317	-0.052662	3.382215
268.750198	3817.797542	16.863322	-0.052690	3.378888
268.584557	3809.832225	16.868327	-0.052654	3.375560
268.240481	3801.851013	16.873331	-0.052585	3.372215
268.597807	3793.826876	16.878336	-0.052647	3.368874
268.347145	3785.856020	16.883341	-0.052595	3.365531
268.174298	3777.898530	16.888346	-0.052557	3.362193
268.146640	3769.889042	16.893351	-0.052547	3.358834
268.156562	3761.861326	16.898355	-0.052544	3.355466
268.114969	3753.873559	16.903360	-0.052531	3.352110
267.862265	3745.894817	16.908365	-0.052479	3.348746
267.787697	3737.874827	16.913370	-0.052460	3.345368
267.936369	3729.920811	16.918375	-0.052482	3.342023
267.868763	3721.917860	16.923379	-0.052465	3.338645
268.009493	3713.912438	16.928384	-0.052486	3.335271
267.682631	3705.931170	16.933389	-0.052420	3.331886
267.518964	3697.932946	16.938394	-0.052384	3.328497
267.668651	3689.951071	16.943399	-0.052407	3.325123
267.669943	3681.993847	16.948403	-0.052402	3.321750
267.566703	3673.999418	16.953408	-0.052378	3.318354
267.555639	3666.009563	16.958413	-0.052371	3.314961
267.407815	3657.976050	16.963418	-0.052338	3.311539
267.371803	3649.980670	16.968423	-0.052326	3.308135
267.129104	3641.980267	16.973427	-0.052276	3.304718
267.262056	3634.034094	16.978432	-0.052296	3.301334
267.213780	3626.047004	16.983437	-0.052281	3.297922
267.083336	3618.063084	16.988442	-0.052252	3.294505
267.043521	3610.053928	16.993447	-0.052239	3.291077
267.158450	3602.047364	16.998451	-0.052256	3.287652
267.302230	3594.046514	17.003456	-0.052277	3.284228
267.044779	3586.121847	17.008461	-0.052224	3.280817
267.070504	3578.130032	17.013466	-0.052224	3.277385
266.874058	3570.155668	17.018471	-0.052182	3.273948
266.797181	3562.121747	17.023475	-0.052163	3.270486
266.751058	3554.133418	17.028480	-0.052149	3.267042
266.780329	3546.131529	17.033485	-0.052150	3.263590
266.673622	3538.146811	17.038490	-0.052125	3.260138
266.735466	3530.194986	17.043495	-0.052131	3.256702
266.713520	3522.170477	17.048499	-0.052122	3.253229
266.674334	3514.161168	17.053504	-0.052109	3.249757
266.374631	3506.219517	17.058509	-0.052048	3.246301
266.382004	3498.216650	17.063514	-0.052045	3.242826
266.434886	3490.235408	17.068519	-0.052049	3.239359
266.234648	3482.251564	17.073523	-0.052007	3.235877
266.443217	3474.205759	17.078528	-0.052041	3.232381
266.325918	3466.208697	17.083533	-0.052014	3.228889
266.076871	3458.210391	17.088538	-0.051962	3.225387
266.072837	3450.285265	17.093543	-0.051956	3.221924
266.177119	3442.259451	17.098547	-0.051971	3.218417
266.192196	3434.278437	17.103552	-0.051968	3.214922
266.218400	3426.269475	17.108557	-0.051968	3.211412
266.200578	3418.286888	17.113562	-0.051960	3.207907
266.004229	3410.329780	17.118567	-0.051918	3.204403
265.862581	3402.365695	17.123571	-0.051887	3.200893
265.950030	3394.381047	17.128576	-0.051898	3.197381
265.661078	3386.406682	17.133581	-0.051839	3.193853
265.550825	3378.364987	17.138586	-0.051813	3.190300
265.572675	3370.387586	17.143591	-0.051812	3.186776
265.460486	3362.404924	17.148595	-0.051786	3.183240
265.548040	3354.412888	17.153600	-0.051797	3.179705
265.464647	3346.451631	17.158605	-0.051777	3.176172
265.545023	3338.406995	17.163610	-0.051787	3.172605
265.583771	3330.429429	17.168615	-0.051789	3.169062
265.381852	3322.439663	17.173619	-0.051746	3.165500
265.408340	3314.491693	17.178624	-0.051746	3.161961
265.182772	3306.514595	17.183629	-0.051699	3.158396
265.215506	3298.511205	17.188634	-0.051700	3.154825
265.309430	3290.495581	17.193639	-0.051712	3.151247
264.976409	3282.507372	17.198643	-0.051645	3.147660
265.037702	3274.525684	17.203648	-0.051651	3.144088
264.792805	3266.554298	17.208653	-0.051600	3.140503
264.830649	3258.580560	17.213658	-0.051602	3.136926
264.818499	3250.586765	17.218663	-0.051595	3.133333
264.588135	3242.579814	17.223667	-0.051547	3.129720
264.708312	3234.601186	17.228672	-0.051564	3.126132
264.792038	3226.632476	17.233677	-0.051575	3.122542
264.666790	3218.638175	17.238682	-0.051546	3.118927
264.568672	3210.685049	17.243687	-0.051523	3.115328
264.493078	3202.636198	17.248691	-0.051504	3.111683
264.492773	3194.656169	17.253696	-0.051499	3.108068
264.213320	3186.692494	17.258701	-0.051441	3.104443
264.218897	3178.700988	17.263706	-0.051437	3.100814
264.660992	3170.731621	17.268711	-0.051515	3.097211
264.419003	3162.723063	17.273715	-0.051464	3.093555
264.139898	3154.734657	17.278720	-0.051407	3.089902
264.032243	3146.774221	17.283725	-0.051382	3.086265
264.058592	3138.776300	17.288730	-0.051382	3.082613
264.145375	3130.794728	17.293735	-0.051393	3.078967
263.949454	3122.820401	17.298739	-0.051351	3.075307
263.933073	3114.747695	17.303744	-0.051343	3.071605
263.944679	3106.755316	17.308749	-0.051340	3.067937
263.653551	3098.796396	17.313754	-0.051281	3.064267
263.996593	3090.818685	17.318759	-0.051340	3.060612
263.698358	3082.869536	17.323763	-0.051279	3.056937
263.468649	3074.900112	17.328768	-0.051231	3.053251
263.546720	3066.863038	17.333773	-0.051241	3.049543
263.577772	3058.883706	17.338778	-0.051241	3.045856
263.619505	3050.943935	17.343783	-0.051244	3.042183
263.589629	3042.954438	17.348787	-0.051233	3.038479
263.670512	3034.974730	17.353792	-0.051243	3.034780
263.489463	3026.957847	17.358797	-0.051204	3.031047
263.332682	3018.983309	17.363802	-0.051170	3.027330
263.405534	3011.007603	17.368807	-0.051179	3.023620
263.410337	3002.997856	17.373811	-0.051174	3.019885
263.129092	2995.074524	17.378816	-0.051117	3.016172
263.117828	2987.066905	17.383821	-0.051110	3.012429
263.054925	2979.059967	17.388826	-0.051093	3.008678
263.023431	2971.091059	17.393831	-0.051082	3.004943
262.889484	2963.134825	17.398835	-0.051052	3.001203
262.883236	2955.161237	17.403840	-0.051046	2.997457
262.884028	2947.144479	17.408845	-0.051041	2.993686
262.717824	2939.122943	17.413850	-0.051004	2.989900
262.919074	2931.139723	17.418855	-0.051037	2.986146
262.603335	2923.191335	17.423859	-0.050973	2.982377
262.680655	2915.189109	17.428864	-0.050982	2.978598
262.758289	2907.216740	17.433869	-0.050992	2.974828
262.537584	2899.227550	17.438874	-0.050945	2.971030
262.326702	2891.275916	17.443879	-0.050901	2.967246
262.213154	2883.284762	17.448883	-0.050875	2.963443
262.502558	2875.272678	17.453888	-0.050923	2.959646
262.499408	2867.341989	17.458893	-0.050918	2.955868
262.260819	2859.334841	17.463898	-0.050868	2.952036
262.311527	2851.353519	17.468903	-0.050873	2.948227
262.077381	2843.357037	17.473907	-0.050824	2.944390
262.114504	2835.394629	17.478912	-0.050826	2.940579
262.198126	2827.425790	17.483917	-0.050836	2.936763
262.183962	2819.408315	17.488922	-0.050828	2.932913
261.948209	2811.444216	17.493927	-0.050779	2.929072
261.794882	2803.463592	17.498931	-0.050746	2.925222
261.801150	2795.514383	17.503936	-0.050742	2.921391
261.776548	2787.537593	17.508941	-0.050732	2.917539
261.744642	2779.499199	17.513946	-0.050721	2.913653
261.765145	2771.457436	17.518951	-0.050720	2.909762
261.638908	2763.491426	17.523955	-0.050691	2.905895
261.388367	2755.568378	17.528960	-0.050639	2.902037
261.422130	2747.577865	17.533965	-0.050641	2.898157
261.445782	2739.572218	17.538970	-0.050640	2.894263
261.463017	2731.610699	17.543975	-0.050638	2.890385
261.360333	2723.621950	17.548979	-0.050614	2.886482
261.593885	2715.646425	17.553984	-0.050652	2.882599
261.224864	2707.719026	17.558989	-0.050578	2.878701
260.976476	2699.749668	17.563994	-0.050527	2.874784
261.097247	2691.713323	17.568999	-0.050544	2.870848
261.088890	2683.743617	17.574003	-0.050538	2.866933
260.889144	2675.776369	17.579008	-0.050495	2.863004
260.876570	2667.806191	17.584013	-0.050488	2.859078
260.856331	2659.818097	17.589018	-0.050479	2.855137
260.739643	2651.818393	17.594023	-0.050452	2.851179
260.664766	2643.849127	17.599027	-0.050433	2.847234
260.700377	2635.854562	17.604032	-0.050435	2.843276
260.705578	2627.895927	17.609037	-0.050431	2.839329
260.629620	2619.921098	17.614042	-0.050411	2.835364
260.383973	2611.939674	17.619047	-0.050360	2.831381
260.313738	2603.924033	17.624051	-0.050342	2.827385
260.327063	2595.949672	17.629056	-0.050340	2.823408
260.288197	2587.998726	17.634061	-0.050327	2.819435
260.325732	2580.008505	17.639066	-0.050329	2.815441
260.325991	2572.009569	17.644071	-0.050324	2.811434
260.178261	2564.016577	17.649075	-0.050291	2.807417
260.201617	2556.065184	17.654080	-0.050291	2.803424
260.036058	2548.121368	17.659085	-0.050255	2.799418
260.098429	2540.153507	17.664090	-0.050261	2.795408
260.160804	2532.139532	17.669095	-0.050268	2.791369
260.086894	2524.141117	17.674099	-0.050249	2.787324
259.795523	2516.191823	17.679104	-0.050190	2.783285
259.733638	2508.238123	17.684109	-0.050173	2.779251
260.009221	2500.207677	17.689114	-0.050219	2.775192
260.078200	2492.230629	17.694119	-0.050227	2.771143
259.807770	2484.286311	17.699123	-0.050171	2.767084
259.808846	2476.323373	17.704128	-0.050166	2.763026
259.658982	2468.378755	17.709133	-0.050134	2.758962
259.473178	2460.410459	17.714138	-0.050094	2.754878
259.629784	2452.330481	17.719143	-0.050118	2.750751
259.372986	2444.368856	17.724147	-0.050065	2.746653
259.304226	2436.418417	17.729152	-0.050047	2.742567
259.372709	2428.433372	17.734157	-0.050055	2.738465
259.208613	2420.460421	17.739162	-0.050019	2.734349
259.269932	2412.478987	17.744167	-0.050025	2.730236
259.105056	2404.519397	17.749171	-0.049989	2.726114
259.111060	2396.563142	17.754176	-0.049986	2.721999
259.169561	2388.593416	17.759181	-0.049991	2.717873
259.128460	2380.607320	17.764186	-0.049979	2.713726
259.159371	2372.615871	17.769191	-0.049979	2.709575
259.022536	2364.646472	17.774195	-0.049949	2.705418
258.939084	2356.694387	17.779200	-0.049928	2.701268
258.829047	2348.733255	17.784205	-0.049902	2.697104
258.592367	2340.749547	17.789210	-0.049853	2.692914
258.633380	2332.761137	17.794215	-0.049856	2.688733
258.668370	2324.772174	17.799219	-0.049857	2.684544
258.427981	2316.852578	17.804224	-0.049807	2.680369
258.640306	2308.871275	17.809229	-0.049842	2.676182
258.506797	2300.864812	17.814234	-0.049812	2.671954
258.579952	2292.869721	17.819239	-0.049820	2.667738
258.418141	2284.902728	17.824243	-0.049785	2.663516
258.402600	2276.941890	17.829248	-0.049777	2.659299
258.455452	2268.984190	17.834253	-0.049782	2.655082
258.333383	2260.987593	17.839258	-0.049754	2.650826
258.445809	2253.030111	17.844263	-0.049770	2.646600
258.003861	2245.085121	17.849267	-0.049682	2.642337
257.893602	2237.127511	17.854272	-0.049657	2.638082
258.071110	2229.138478	17.859277	-0.049685	2.633822
257.888549	2221.142110	17.864282	-0.049646	2.629527
257.770757	2213.218401	17.869287	-0.049619	2.625269
257.851214	2205.225424	17.874291	-0.049628	2.620980
257.726018	2197.261288	17.879296	-0.049600	2.616686
257.510761	2189.287282	17.884301	-0.049555	2.612373
257.361915	2181.298705	17.889306	-0.049522	2.608050
257.405640	2173.336502	17.894311	-0.049525	2.603746
257.263763	2165.385427	17.899315	-0.049494	2.599429
257.391005	2157.416476	17.904320	-0.049512	2.595114
257.441352	2149.246176	17.909325	-0.049516	2.590676
257.268833	2141.292087	17.914330	-0.049479	2.586334
257.184924	2133.388428	17.919335	-0.049458	2.582017
257.120485	2125.445919	17.924339	-0.049441	2.577674
257.022745	2117.489368	17.929344	-0.049418	2.573313
257.063046	2109.517368	17.934349	-0.049420	2.568946
256.970458	2101.540946	17.939354	-0.049398	2.564560
257.080778	2093.616192	17.944359	-0.049414	2.560208
256.724505	2085.699416	17.949363	-0.049342	2.555822
256.676306	2077.697912	17.954368	-0.049328	2.551402
256.796814	2069.714346	17.959373	-0.049345	2.546996
256.734242	2061.747432	17.964378	-0.049329	2.542579
256.479931	2053.831089	17.969383	-0.049276	2.538169
256.338608	2045.848913	17.974387	-0.049245	2.533723
256.384319	2037.850585	17.979392	-0.049248	2.529273
256.326342	2029.895732	17.984397	-0.049232	2.524832
256.220165	2021.954359	17.989402	-0.049207	2.520388
256.200695	2014.000921	17.994407	-0.049199	2.515934
256.042364	2005.990344	17.999411	-0.049164	2.511431
255.974046	1998.025717	18.004416	-0.049146	2.506953
256.164321	1990.041873	18.009421	-0.049177	2.502474
256.167468	1982.078561	18.014426	-0.049172	2.497985
256.064754	1974.143467	18.019431	-0.049148	2.493496
255.934538	1966.161765	18.024435	-0.049118	2.488971
255.713283	1958.217146	18.029440	-0.049072	2.484451
255.807434	1950.256463	18.034445	-0.049085	2.479938
255.715772	1942.314823	18.039450	-0.049062	2.475413
255.660153	1934.322599	18.044455	-0.049047	2.470854
255.454349	1926.372323	18.049459	-0.049004	2.466299
255.543934	1918.391315	18.054464	-0.049015	2.461741
255.488166	1910.463842	18.059469	-0.049000	2.457193
255.284598	1902.488611	18.064474	-0.048957	2.452599
255.211911	1894.529766	18.069479	-0.048938	2.448015
255.269892	1886.543861	18.074483	-0.048944	2.443417
255.434816	1878.572422	18.079488	-0.048969	2.438827
255.413353	1870.626880	18.084493	-0.048960	2.434229
255.073649	1862.616866	18.089498	-0.048892	2.429560
255.104212	1854.657470	18.094503	-0.048892	2.424941
254.927098	1846.728817	18.099507	-0.048854	2.420314
254.849255	1838.776097	18.104512	-0.048835	2.415672
254.914504	1830.801883	18.109517	-0.048842	2.411020
254.845787	1822.824252	18.114522	-0.048824	2.406346
254.724277	1814.914909	18.119527	-0.048796	2.401699
254.612826	1806.968638	18.124531	-0.048770	2.397022
254.598979	1798.980176	18.129536	-0.048763	2.392319
254.595618	1791.027707	18.134541	-0.048757	2.387628
254.565800	1783.043986	18.139546	-0.048746	2.382908
254.590060	1775.118906	18.144551	-0.048746	2.378217
254.546173	1767.143121	18.149555	-0.048733	2.373482
254.292430	1759.191469	18.154560	-0.048680	2.368734
254.388477	1751.242988	18.159565	-0.048693	2.364007
254.232240	1743.307934	18.164570	-0.048659	2.359259
254.315476	1735.344452	18.169575	-0.048669	2.354503
254.008888	1727.371233	18.174579	-0.048607	2.349700
254.016099	1719.392134	18.179584	-0.048603	2.344909
254.117558	1711.446902	18.184589	-0.048617	2.340136
253.860359	1703.517231	18.189594	-0.048564	2.335333
254.007654	1695.537566	18.194599	-0.048586	2.330524
253.961380	1687.577372	18.199603	-0.048573	2.325700
253.640031	1679.667521	18.204608	-0.048508	2.320875
253.532073	1671.741161	18.209613	-0.048483	2.316047
253.421515	1663.749078	18.214618	-0.048457	2.311168
253.554235	1655.779526	18.219623	-0.048477	2.306313
253.454822	1647.821958	18.224627	-0.048453	2.301436
253.383316	1639.907501	18.229632	-0.048435	2.296577
253.452028	1631.924362	18.234637	-0.048442	2.291678
253.263046	1623.980969	18.239642	-0.048402	2.286770
253.274255	1616.042117	18.244647	-0.048399	2.281872
253.220911	1608.103463	18.249651	-0.048384	2.276958
253.203209	1600.086229	18.254656	-0.048376	2.271988
253.305186	1592.097622	18.259661	-0.048389	2.267035
253.218339	1584.157769	18.264666	-0.048368	2.262085
252.904406	1576.277293	18.269671	-0.048305	2.257141
252.860177	1568.309289	18.274675	-0.048291	2.252156
252.767499	1560.358459	18.279680	-0.048269	2.247165
252.841743	1552.419006	18.284685	-0.048278	2.242186
252.485267	1544.515253	18.289690	-0.048206	2.237180
252.559068	1536.537770	18.294695	-0.048215	2.232154
252.712767	1528.539900	18.299699	-0.048238	2.227111
252.446202	1520.636522	18.304704	-0.048184	2.222079
252.487908	1512.697239	18.309709	-0.048186	2.217040
252.253897	1504.744335	18.314714	-0.048138	2.211956
252.499534	1496.766690	18.319719	-0.048178	2.206888
252.210660	1488.882356	18.324723	-0.048120	2.201820
252.208962	1480.941136	18.329728	-0.048114	2.196730
251.948401	1472.991477	18.334733	-0.048061	2.191599
252.070834	1464.996833	18.339738	-0.048078	2.186461
252.153329	1457.057922	18.344743	-0.048088	2.181344
251.891651	1449.150640	18.349747	-0.048035	2.176204
252.009537	1441.167759	18.354752	-0.048052	2.171037
251.979721	1433.228350	18.359757	-0.048041	2.165873
251.754413	1425.319170	18.364762	-0.047994	2.160698
251.731629	1417.399293	18.369767	-0.047985	2.155522
251.656613	1409.424931	18.374771	-0.047966	2.150294
251.431423	1401.511868	18.379776	-0.047919	2.145078
251.625889	1393.550617	18.384781	-0.047950	2.139858
251.561287	1385.617357	18.389786	-0.047933	2.134619
251.505703	1377.674959	18.394791	-0.047917	2.129362
251.495994	1369.739497	18.399795	-0.047910	2.124101
251.505699	1361.811273	18.404800	-0.047907	2.118833
251.308839	1353.887772	18.409805	-0.047865	2.113536
251.375460	1345.858517	18.414810	-0.047872	2.108180
251.118464	1337.975700	18.419815	-0.047820	2.102877
251.044547	1330.046534	18.424819	-0.047801	2.097547
251.046772	1322.099664	18.429824	-0.047796	2.092199
250.982581	1314.168620	18.434829	-0.047779	2.086842
250.864652	1306.246637	18.439834	-0.047752	2.081471
250.800515	1298.345397	18.444839	-0.047735	2.076107
250.773910	1290.379359	18.449843	-0.047725	2.070687
250.699320	1282.440477	18.454848	-0.047706	2.065268
250.582149	1274.541223	18.459853	-0.047679	2.059857
250.491703	1266.604069	18.464858	-0.047657	2.054408
250.632953	1258.652544	18.469863	-0.047678	2.048958
250.470121	1250.730145	18.474867	-0.047643	2.043483
250.298916	1242.842494	18.479872	-0.047606	2.038017
250.416589	1234.882837	18.484877	-0.047623	2.032515
250.229749	1226.941135	18.489882	-0.047583	2.026980
250.208946	1219.024109	18.494887	-0.047574	2.021464
250.125524	1211.108453	18.499891	-0.047553	2.015927
250.175560	1203.147029	18.504896	-0.047558	2.010356
249.922733	1195.270569	18.509901	-0.047506	2.004799
249.885363	1187.341297	18.514906	-0.047494	1.999211
249.809833	1179.431464	18.519911	-0.047474	1.993617
249.656809	1171.491532	18.524915	-0.047441	1.987978
249.631666	1163.564443	18.529920	-0.047431	1.982345
249.520535	1155.676389	18.534925	-0.047405	1.976715
249.309602	1147.746737	18.539930	-0.047361	1.971029
249.303988	1139.816450	18.544935	-0.047355	1.965347
249.564271	1131.883244	18.549939	-0.047398	1.959676
249.472937	1123.960226	18.554944	-0.047376	1.953958
249.339280	1116.026016	18.559949	-0.047346	1.948210
249.142187	1108.116640	18.564954	-0.047304	1.942456
249.242744	1100.189580	18.569959	-0.047318	1.936704
249.119452	1092.280477	18.574963	-0.047290	1.930925
248.961029	1084.363328	18.579968	-0.047255	1.925117
249.022319	1076.465106	18.584973	-0.047262	1.919331
248.797109	1068.565210	18.589978	-0.047215	1.913494
248.841944	1060.622587	18.594983	-0.047218	1.907638
248.794878	1052.716501	18.599987	-0.047204	1.901780
248.639716	1044.825754	18.604992	-0.047170	1.895903
248.565470	1036.915911	18.609997	-0.047151	1.890003
248.322106	1029.030612	18.615002	-0.047101	1.884084
248.389515	1021.128005	18.620007	-0.047109	1.878168
248.224649	1013.217991	18.625011	-0.047073	1.872202
248.239811	1005.264948	18.630016	-0.047071	1.866205
248.173183	997.379147	18.635021	-0.047053	1.860229
248.261210	989.454012	18.640026	-0.047064	1.854223
248.186384	981.559921	18.645031	-0.047045	1.848202
247.939212	973.677401	18.650035	-0.046994	1.842149
247.955699	965.772594	18.655040	-0.046992	1.836091
247.992726	957.860075	18.660045	-0.046994	1.830009
247.736079	949.989669	18.665050	-0.046941	1.823904
247.912815	942.064180	18.670055	-0.046969	1.817788
247.714122	934.193158	18.675059	-0.046927	1.811649
247.526883	926.298016	18.680064	-0.046887	1.805471
247.607355	918.413149	18.685069	-0.046897	1.799312
247.464765	910.508488	18.690074	-0.046866	1.793090
247.422715	902.569089	18.695079	-0.046853	1.786831
247.278160	894.701791	18.700083	-0.046821	1.780594
247.319189	886.806212	18.705088	-0.046823	1.774335
247.372218	878.895238	18.710093	-0.046828	1.768044
247.172507	871.037831	18.715098	-0.046786	1.761742
247.089508	863.173772	18.720103	-0.046765	1.755426
247.107917	855.258510	18.725107	-0.046764	1.749059
247.001053	847.378849	18.730112	-0.046739	1.742681
246.818285	839.538807	18.735117	-0.046700	1.736303
246.634966	831.661331	18.740122	-0.046661	1.729870
246.505880	823.790656	18.745127	-0.046632	1.723426
246.489982	815.924301	18.750131	-0.046624	1.716976
246.662140	807.981965	18.755136	-0.046651	1.710463
246.602576	800.113871	18.760141	-0.046634	1.703957
246.165699	792.291899	18.765146	-0.046548	1.697414
246.251421	784.381671	18.770151	-0.046559	1.690842
246.183858	776.508192	18.775155	-0.046541	1.684254
246.087856	768.653870	18.780160	-0.046518	1.677652
246.157155	760.765285	18.785165	-0.046526	1.671018
246.122851	752.888216	18.790170	-0.046515	1.664353
245.914180	745.060816	18.795175	-0.046471	1.657680
245.733775	737.204302	18.800179	-0.046432	1.650958
245.790108	729.314739	18.805184	-0.046438	1.644214
245.833004	721.476968	18.810189	-0.046441	1.637484
245.463225	713.608983	18.815194	-0.046367	1.630643
245.728244	705.692526	18.820199	-0.046411	1.623820
245.810565	697.833383	18.825203	-0.046421	1.616992
245.404090	690.022804	18.830208	-0.046341	1.610109
245.415160	682.176209	18.835213	-0.046338	1.603224
245.183826	674.356906	18.840218	-0.046290	1.596299
245.076915	666.498058	18.845223	-0.046265	1.589326
245.133078	658.634717	18.850227	-0.046270	1.582342
245.186231	650.778191	18.855232	-0.046275	1.575332
245.127832	642.943931	18.860237	-0.046259	1.568295
244.886852	635.133340	18.865242	-0.046209	1.561221
244.687157	627.331536	18.870247	-0.046167	1.554129
244.587259	619.475016	18.875251	-0.046144	1.546969
244.400432	611.649382	18.880256	-0.046104	1.539791
244.524697	603.804810	18.885261	-0.046122	1.532608
244.417669	595.957015	18.890266	-0.046097	1.525354
244.447651	588.141282	18.895271	-0.046097	1.518116
244.435975	580.303589	18.900275	-0.046090	1.510816
244.238151	572.491100	18.905280	-0.046048	1.503476
244.377252	564.666892	18.910285	-0.046069	1.496140
243.979832	556.889181	18.915290	-0.045990	1.488730
243.854636	549.089816	18.920295	-0.045962	1.481304
243.981751	541.247186	18.925299	-0.045981	1.473838
243.901331	533.387004	18.930304	-0.045961	1.466285
243.711628	525.626910	18.935309	-0.045920	1.458773
243.601064	517.823878	18.940314	-0.045895	1.451192
243.475507	510.037749	18.945319	-0.045866	1.443586
243.516436	502.245416	18.950323	-0.045869	1.435960
243.372836	494.442215	18.955328	-0.045837	1.428252
243.299725	486.664534	18.960333	-0.045819	1.420540
243.153876	478.890110	18.965338	-0.045787	1.412776
243.159123	471.082945	18.970343	-0.045783	1.404962
243.165723	463.315922	18.975347	-0.045779	1.397145
242.865959	455.548931	18.980352	-0.045718	1.389233
242.993328	447.753096	18.985357	-0.045737	1.381318
242.786487	440.002015	18.990362	-0.045693	1.373346
242.879482	432.206745	18.995367	-0.045706	1.365334
242.678572	424.490010	19.000371	-0.045663	1.357305
242.354120	416.755746	19.005376	-0.045598	1.349188
242.684253	408.933278	19.010381	-0.045654	1.341044
242.411456	401.223470	19.015386	-0.045599	1.332863
242.174588	393.503168	19.020391	-0.045550	1.324627
242.083137	385.778437	19.025395	-0.045528	1.316360
241.953867	377.907895	19.030400	-0.045499	1.307877
241.909024	370.182632	19.035405	-0.045485	1.299512
241.830930	362.458943	19.040410	-0.045466	1.291088
241.779471	354.744996	19.045415	-0.045451	1.282624
241.651910	347.052597	19.050419	-0.045423	1.274114
241.532040	339.333409	19.055424	-0.045395	1.265518
241.546093	331.629794	19.060429	-0.045393	1.256906
241.436167	323.928992	19.065434	-0.045368	1.248214
241.390506	316.242602	19.070439	-0.045354	1.239490
241.385262	308.536134	19.075443	-0.045348	1.230689
241.048217	300.881711	19.080448	-0.045281	1.221819
241.043206	293.205678	19.085453	-0.045275	1.212925
240.998746	285.520825	19.090458	-0.045262	1.203948
241.036162	277.848796	19.095463	-0.045264	1.194934
240.740754	270.222097	19.100467	-0.045204	1.185838
240.612073	262.580226	19.105472	-0.045175	1.176687
240.693074	254.911005	19.110477	-0.045185	1.167475
240.311944	247.329256	19.115482	-0.045109	1.158200
239.993165	239.703190	19.120487	-0.045045	1.148809
240.044615	232.041313	19.125491	-0.045050	1.139374
239.953209	224.415635	19.130496	-0.045028	1.129876
239.866444	216.811452	19.135501	-0.045007	1.120324
239.685288	209.229390	19.140506	-0.044968	1.110698
239.953365	201.576780	19.145511	-0.045013	1.100996
239.806646	194.021244	19.150515	-0.044981	1.091242
239.625688	186.464693	19.155520	-0.044943	1.081390
239.398103	178.936398	19.160525	-0.044895	1.071474
239.278738	171.372276	19.165530	-0.044868	1.061443
239.167807	163.838647	19.170535	-0.044843	1.051358
239.041018	156.314861	19.175539	-0.044814	1.041186
238.736525	148.828718	19.180544	-0.044753	1.030922
238.589534	141.328098	19.185549	-0.044721	1.020573
238.279825	133.857783	19.190554	-0.044658	1.010121
238.421449	126.338119	19.195559	-0.044680	0.999600
237.985860	118.896653	19.200563	-0.044594	0.988936
237.419081	111.497026	19.205568	-0.044484	0.978182
237.019208	104.090854	19.210573	-0.044405	0.967342
236.354911	96.745461	19.215578	-0.044276	0.956400
235.891664	89.361759	19.220583	-0.044185	0.945326
235.344051	82.017692	19.225587	-0.044079	0.934158
234.700353	74.685574	19.230592	-0.043954	0.922848
234.393425	67.326236	19.235597	-0.043892	0.911446
233.724539	60.259210	19.240602	-0.043763	0.900257