Tue Mar 23 11:30:21 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.791189	-0.009510	0.000000	-0.000009	0.723011

0.940063	-0.030824	0.005005	-0.000037	0.723022
0.893574	-0.027941	0.010010	-0.000028	0.723011
0.830961	-0.139700	0.015014	-0.000017	0.722770
0.742855	-0.157278	0.020019	-0.000000	0.722705
0.601147	-0.135493	0.025024	0.000026	0.722699
0.746048	-0.157375	0.030029	-0.000001	0.722707
0.670233	-0.146248	0.035034	0.000013	0.722702
0.830981	-0.175881	0.040038	-0.000017	0.722700
0.699650	-0.148231	0.045043	0.000007	0.722709
0.545086	-0.125629	0.050048	0.000036	0.722700
0.802370	-0.167716	0.055053	-0.000012	0.722707
0.783026	-0.166920	0.060058	-0.000009	0.722702
0.655042	-0.145153	0.065062	0.000015	0.722700
0.827718	-0.174882	0.070067	-0.000017	0.722702
0.615696	-0.140740	0.075072	0.000022	0.722696
0.868349	-0.307257	0.080077	-0.000025	0.722457
0.972079	-0.365607	0.085082	-0.000044	0.722379
0.763425	-0.328167	0.090086	-0.000006	0.722380
0.693362	-0.312578	0.095091	0.000007	0.722386
0.544299	-0.290834	0.100096	0.000035	0.722377
0.712635	-0.318480	0.105101	0.000004	0.722382
0.388285	-0.319094	0.110106	0.000064	0.722267
0.455526	-0.425680	0.115110	0.000051	0.722082
0.477014	-0.426589	0.120115	0.000047	0.722087
0.572124	-0.448192	0.125120	0.000029	0.722078
0.788466	-0.483472	0.130125	-0.000011	0.722085
0.766708	-0.520932	0.135130	-0.000007	0.722004
0.668871	-0.633434	0.140134	0.000011	0.721749
0.588132	-0.616185	0.145139	0.000026	0.721755
0.670113	-0.634972	0.150144	0.000011	0.721747
0.761009	-0.653123	0.155149	-0.000006	0.721743
0.501127	-0.756613	0.160154	0.000042	0.721449
0.579950	-0.772218	0.165158	0.000027	0.721446
0.703528	-0.792139	0.170163	0.000004	0.721450
0.622210	-0.828204	0.175168	0.000019	0.721351
0.626947	-0.937349	0.180173	0.000018	0.721138
0.613739	-0.937044	0.185178	0.000021	0.721134
0.591475	-0.934730	0.190182	0.000025	0.721131
0.492084	-1.026374	0.195187	0.000043	0.720916
0.717961	-1.083903	0.200192	0.000001	0.720882
0.765032	-1.087548	0.205197	-0.000008	0.720892
0.711579	-1.225472	0.210202	0.000002	0.720602
0.511620	-1.217047	0.215206	0.000039	0.720549
0.617558	-1.233435	0.220211	0.000019	0.720554
0.629556	-1.392531	0.225216	0.000017	0.720245
0.564421	-1.386940	0.230221	0.000029	0.720233
0.491521	-1.412533	0.235226	0.000043	0.720157
0.538056	-1.548228	0.240230	0.000034	0.719906
0.196766	-1.484276	0.245235	0.000097	0.719913
0.226923	-1.577974	0.250240	0.000092	0.719739
0.413167	-1.673316	0.255245	0.000057	0.719617
0.168567	-1.632558	0.260250	0.000102	0.719611
-0.080282	-1.756001	0.265254	0.000149	0.719281
0.198793	-1.802749	0.270259	0.000097	0.719287
0.217115	-1.887973	0.275264	0.000093	0.719125
0.040447	-1.932248	0.280269	0.000126	0.718976
0.159850	-1.974574	0.285274	0.000104	0.718935
0.106163	-2.105608	0.290278	0.000114	0.718657
0.174495	-2.116100	0.295283	0.000101	0.718661
0.141682	-2.243408	0.300288	0.000107	0.718398
0.143282	-2.258141	0.305293	0.000107	0.718370
0.130633	-2.375712	0.310298	0.000109	0.718133
-0.319931	-2.348908	0.315302	0.000193	0.718028
-0.156710	-2.459238	0.320307	0.000162	0.717868
-3.119231	-2.014654	0.325312	0.000713	0.717704
-1.929684	-2.221104	0.330317	0.000492	0.717715
-2.220399	-2.285292	0.335322	0.000546	0.717486
-3.926596	-2.032259	0.340326	0.000863	0.717385
-3.210773	-2.156642	0.345331	0.000730	0.717392
-2.952007	-2.276100	0.350336	0.000682	0.717247
-4.335863	-2.106365	0.355341	0.000939	0.717095
-4.017662	-2.164516	0.360346	0.000880	0.717092
-4.077730	-2.155459	0.365350	0.000891	0.717089
-4.680849	-2.203014	0.370355	0.001003	0.716783
-5.412122	-2.085538	0.375360	0.001139	0.716758
-5.099248	-2.138128	0.380365	0.001081	0.716764
-4.657144	-2.218110	0.385370	0.000999	0.716762
-5.583799	-2.200126	0.390374	0.001171	0.716471
-6.261577	-2.084958	0.395379	0.001297	0.716460
-6.122260	-2.112276	0.400384	0.001271	0.716455
-5.953491	-2.139323	0.405389	0.001240	0.716462
-6.273471	-2.124522	0.410394	0.001299	0.716378
-6.976727	-2.119612	0.415398	0.001430	0.716140
-6.388077	-2.222347	0.420403	0.001320	0.716144
-7.374409	-2.052022	0.425408	0.001504	0.716134
-6.946657	-2.123857	0.430413	0.001424	0.716143
-6.759396	-2.191854	0.435418	0.001389	0.716074
-8.233315	-2.024037	0.440422	0.001663	0.715887
-7.709528	-2.112310	0.445427	0.001566	0.715897
-7.700533	-2.118661	0.450432	0.001564	0.715888
-7.911968	-2.077996	0.455437	0.001603	0.715894
-7.815514	-2.097246	0.460442	0.001585	0.715890
-8.239619	-2.147946	0.465446	0.001664	0.715640
-8.619613	-2.120907	0.470451	0.001735	0.715560
-8.939238	-2.070694	0.475456	0.001794	0.715546
-8.831508	-2.085694	0.480461	0.001774	0.715555
-8.759440	-2.100522	0.485466	0.001760	0.715551
-8.640534	-2.122472	0.490470	0.001738	0.715550
-9.005155	-2.186417	0.495475	0.001806	0.715294
-10.049221	-2.029355	0.500480	0.002000	0.715237
-9.633176	-2.100334	0.505485	0.001922	0.715244
-9.492370	-2.128309	0.510490	0.001896	0.715238
-9.855301	-2.064242	0.515494	0.001964	0.715237
-9.419387	-2.138170	0.520499	0.001882	0.715245
-9.929279	-2.151210	0.525504	0.001977	0.715039
-10.754857	-2.062462	0.530509	0.002131	0.714923
-10.256357	-2.154737	0.535514	0.002038	0.714917
-10.618325	-2.091350	0.540518	0.002105	0.714915
-10.884242	-2.039960	0.545523	0.002155	0.714923
-10.577897	-2.100211	0.550528	0.002097	0.714912
-10.526416	-2.111882	0.555533	0.002088	0.714907
-11.476232	-2.089075	0.560538	0.002264	0.714617
-11.734705	-2.044042	0.565542	0.002312	0.714615
-11.405387	-2.098873	0.570547	0.002251	0.714623
-11.382296	-2.107608	0.575552	0.002247	0.714614
-11.712943	-2.045632	0.580557	0.002308	0.714620
-11.610397	-2.065022	0.585562	0.002289	0.714618
-11.353495	-2.117801	0.590566	0.002241	0.714604
-11.917351	-2.174202	0.595571	0.002346	0.714293
-12.670899	-2.043812	0.600576	0.002486	0.714285
-12.631464	-2.048346	0.605581	0.002479	0.714291
-12.325534	-2.104317	0.610586	0.002422	0.714288
-12.680391	-2.042468	0.615590	0.002487	0.714285
-12.306773	-2.105232	0.620595	0.002418	0.714293
-12.756841	-2.029528	0.625600	0.002502	0.714284
-12.951366	-2.128080	0.630605	0.002538	0.714020
-13.260615	-2.092454	0.635610	0.002595	0.713981
-13.417182	-2.065571	0.640614	0.002624	0.713980
-13.445947	-2.057527	0.645619	0.002629	0.713986
-13.744963	-2.007665	0.650624	0.002685	0.713979
-13.292735	-2.086987	0.655629	0.002601	0.713982
-13.361510	-2.074642	0.660634	0.002613	0.713982
-13.971705	-2.078485	0.665638	0.002727	0.713759
-14.091607	-2.102169	0.670643	0.002749	0.713669
-14.045004	-2.116186	0.675648	0.002740	0.713658
-14.301529	-2.067414	0.680653	0.002788	0.713664
-14.443611	-2.043464	0.685658	0.002814	0.713662
-14.307751	-2.069376	0.690662	0.002789	0.713659
-14.366649	-2.055259	0.695667	0.002800	0.713666
-14.774659	-2.060693	0.700672	0.002876	0.713511
-15.336820	-2.032569	0.705677	0.002980	0.713368
-15.186456	-2.059536	0.710682	0.002952	0.713368
-15.527887	-2.000229	0.715686	0.003016	0.713365
-15.022387	-2.088183	0.720691	0.002921	0.713369
-15.337191	-2.036484	0.725696	0.002980	0.713361
-15.600378	-1.985506	0.730701	0.003029	0.713369
-15.119546	-2.072910	0.735706	0.002939	0.713366
-15.518291	-2.171172	0.740710	0.003013	0.713029
-16.142346	-2.058733	0.745715	0.003129	0.713032
-16.442225	-2.009297	0.750720	0.003185	0.713024
-15.776451	-2.124276	0.755725	0.003061	0.713032
-15.900964	-2.102982	0.760730	0.003084	0.713030
-16.591033	-1.981019	0.765734	0.003212	0.713028
-15.748201	-2.136047	0.770739	0.003055	0.713019
-16.690938	-2.122225	0.775744	0.003231	0.712712
-17.105180	-2.044379	0.780749	0.003308	0.712720
-17.019422	-2.061719	0.785754	0.003292	0.712717
-17.017132	-2.063993	0.790758	0.003291	0.712713
-16.995868	-2.064082	0.795763	0.003287	0.712721
-17.285485	-2.017334	0.800768	0.003341	0.712711
-17.045125	-2.056767	0.805773	0.003296	0.712718
-17.101545	-2.174128	0.810778	0.003307	0.712464
-18.309004	-1.996967	0.815782	0.003531	0.712389
-17.789286	-2.083898	0.820787	0.003434	0.712401
-18.005763	-2.050176	0.825792	0.003475	0.712391
-18.284020	-1.999493	0.830797	0.003526	0.712394
-17.883283	-2.070908	0.835802	0.003452	0.712394
-18.032368	-2.046528	0.840806	0.003479	0.712390
-18.101153	-2.095754	0.845811	0.003492	0.712267
-19.276865	-1.973534	0.850816	0.003711	0.712094
-18.385202	-2.129629	0.855821	0.003545	0.712099
-18.613773	-2.089286	0.860826	0.003587	0.712099
-19.291984	-1.972049	0.865830	0.003713	0.712092
-18.664306	-2.078374	0.870835	0.003596	0.712103
-18.622667	-2.091455	0.875840	0.003588	0.712092
-19.008859	-2.088962	0.880845	0.003660	0.711960
-20.046630	-2.000509	0.885850	0.003853	0.711768
-19.654009	-2.071616	0.890854	0.003780	0.711766
-19.564418	-2.083531	0.895859	0.003763	0.711774
-20.028282	-2.005221	0.900864	0.003850	0.711766
-19.681364	-2.065955	0.905869	0.003785	0.711768
-19.589855	-2.079660	0.910874	0.003768	0.711773
-19.852797	-2.045128	0.915878	0.003817	0.711749
-20.164346	-2.130858	0.920883	0.003875	0.711467
-20.469879	-2.081026	0.925888	0.003931	0.711458
-21.136188	-1.959485	0.930893	0.004055	0.711464
-20.700881	-2.037690	0.935898	0.003974	0.711463
-20.549034	-2.067153	0.940902	0.003946	0.711459
-20.576271	-2.057827	0.945907	0.003951	0.711468
-21.042671	-1.980703	0.950912	0.004037	0.711456
-20.965059	-2.110795	0.955917	0.004023	0.711224
-21.405962	-2.071213	0.960922	0.004105	0.711147
-21.834123	-1.997849	0.965926	0.004184	0.711141
-21.535736	-2.046695	0.970931	0.004129	0.711150
-21.821382	-2.000520	0.975936	0.004182	0.711141
-21.634171	-2.030770	0.980941	0.004147	0.711147
-21.572671	-2.043668	0.985946	0.004135	0.711143
-21.678861	-2.087210	0.990950	0.004155	0.711019
-22.026250	-2.093123	0.995955	0.004220	0.710884
-22.251524	-2.058405	1.000960	0.004261	0.710873
-22.489328	-2.013208	1.005965	0.004306	0.710879
-22.130848	-2.077375	1.010970	0.004239	0.710879
-22.495167	-2.015069	1.015974	0.004306	0.710874
-22.413642	-2.024343	1.020979	0.004291	0.710884
-22.459040	-2.144103	1.025984	0.004300	0.710629
-23.517804	-2.000767	1.030989	0.004496	0.710539
-23.269845	-2.042666	1.035994	0.004450	0.710544
-23.232748	-2.052894	1.040998	0.004443	0.710536
-23.187512	-2.057307	1.046003	0.004435	0.710544
-23.468086	-2.010544	1.051008	0.004487	0.710538
-23.570377	-1.991132	1.056013	0.004506	0.710540
-23.159251	-2.158348	1.061018	0.004429	0.710353
-24.339464	-2.015022	1.066022	0.004649	0.710219
-24.405276	-1.999533	1.071027	0.004661	0.710227
-24.177335	-2.043452	1.076032	0.004618	0.710220
-24.390513	-2.003384	1.081037	0.004658	0.710225
-24.099125	-2.057006	1.086042	0.004604	0.710222
-24.453742	-1.996307	1.091046	0.004669	0.710217
-24.138815	-2.108706	1.096051	0.004611	0.710105
-25.292426	-2.007833	1.101056	0.004825	0.709895
-25.095505	-2.039121	1.106061	0.004789	0.709903
-24.874265	-2.078995	1.111066	0.004747	0.709903
-25.351638	-1.996616	1.116070	0.004836	0.709897
-25.068073	-2.043575	1.121075	0.004783	0.709905
-25.082090	-2.045513	1.126080	0.004786	0.709896
-25.118465	-2.069263	1.131085	0.004792	0.709836
-25.787973	-2.064590	1.136090	0.004917	0.709607
-26.080195	-2.015433	1.141094	0.004971	0.709601
-25.887320	-2.046235	1.146099	0.004935	0.709608
-26.035323	-2.025038	1.151104	0.004963	0.709598
-25.962172	-2.037980	1.156109	0.004949	0.709599
-25.884996	-2.049962	1.161114	0.004934	0.709602
-26.235222	-2.010637	1.166118	0.005000	0.709556
-26.828340	-2.047094	1.171123	0.005110	0.709272
-26.847108	-2.047986	1.176128	0.005113	0.709264
-26.936611	-2.028358	1.181133	0.005130	0.709272
-26.676297	-2.075430	1.186138	0.005081	0.709270
-27.093660	-2.003465	1.191142	0.005159	0.709266
-26.600930	-2.086297	1.196147	0.005067	0.709276
-26.820304	-2.066962	1.201152	0.005108	0.709237
-27.826564	-2.025523	1.206157	0.005295	0.708961
-27.615271	-2.062887	1.211162	0.005256	0.708962
-27.767787	-2.037060	1.216166	0.005284	0.708959
-27.659549	-2.053877	1.221171	0.005264	0.708964
-28.000552	-1.997113	1.226176	0.005327	0.708956
-28.078907	-1.981656	1.231181	0.005341	0.708960
-27.589891	-2.067260	1.236186	0.005250	0.708963
-27.922342	-2.140144	1.241190	0.005312	0.708698
-28.418861	-2.074949	1.246195	0.005404	0.708652
-28.683924	-2.032533	1.251200	0.005454	0.708643
-28.753671	-2.017519	1.256205	0.005467	0.708648
-28.515314	-2.060252	1.261210	0.005422	0.708648
-28.552330	-2.057070	1.266214	0.005429	0.708641
-28.661426	-2.041511	1.271219	0.005449	0.708633
-29.535468	-2.026423	1.276224	0.005612	0.708352
-29.492056	-2.031770	1.281229	0.005604	0.708357
-29.712906	-1.992984	1.286234	0.005645	0.708356
-29.806841	-1.979658	1.291238	0.005662	0.708349
-29.630272	-2.007409	1.296243	0.005629	0.708357
-29.519880	-2.028780	1.301248	0.005608	0.708354
-29.691500	-1.996782	1.306253	0.005640	0.708357
-29.434442	-2.134227	1.311258	0.005592	0.708173
-30.701805	-1.988628	1.316262	0.005828	0.708012
-30.276943	-2.058955	1.321267	0.005749	0.708023
-30.224823	-2.074456	1.326272	0.005739	0.708011
-30.645743	-1.997448	1.331277	0.005817	0.708015
-30.311857	-2.054093	1.336282	0.005755	0.708021
-30.433262	-2.038710	1.341286	0.005778	0.708009
-30.513500	-2.125962	1.346291	0.005792	0.707806
-31.581003	-1.988818	1.351296	0.005991	0.707699
-31.586225	-1.986317	1.356301	0.005992	0.707703
-31.227164	-2.050057	1.361306	0.005925	0.707703
-31.411673	-2.018213	1.366310	0.005959	0.707701
-31.551945	-1.990206	1.371315	0.005985	0.707708
-31.431718	-2.015313	1.376320	0.005963	0.707700
-31.332297	-2.081601	1.381325	0.005944	0.707603
-32.312466	-2.015726	1.386330	0.006126	0.707385
-32.193564	-2.041451	1.391334	0.006104	0.707376
-32.082978	-2.058073	1.396339	0.006084	0.707383
-32.109335	-2.055967	1.401344	0.006088	0.707378
-32.114367	-2.053540	1.406349	0.006089	0.707381
-32.146766	-2.044953	1.411354	0.006095	0.707387
-32.343580	-2.077904	1.416358	0.006132	0.707250
-33.244554	-1.997438	1.421363	0.006299	0.707090
-33.037571	-2.036721	1.426368	0.006261	0.707085
-33.248949	-1.996666	1.431373	0.006300	0.707090
-33.217760	-2.003143	1.436378	0.006294	0.707088
-33.238063	-2.002504	1.441382	0.006298	0.707083
-32.696170	-2.095254	1.446387	0.006197	0.707091
-32.921522	-2.125227	1.451392	0.006239	0.706950
-34.320682	-1.971359	1.456397	0.006499	0.706758
-33.837621	-2.057475	1.461402	0.006409	0.706758
-33.995857	-2.033650	1.466406	0.006438	0.706750
-34.297505	-1.974710	1.471411	0.006494	0.706761
-34.017581	-2.029285	1.476416	0.006442	0.706751
-33.907112	-2.046356	1.481421	0.006421	0.706757
-33.833478	-2.097184	1.486426	0.006408	0.706681
-35.116565	-1.986520	1.491430	0.006646	0.706444
-34.722323	-2.051139	1.496435	0.006573	0.706456
-34.896857	-2.025883	1.501440	0.006605	0.706444
-34.742721	-2.051437	1.506445	0.006576	0.706448
-34.636075	-2.070119	1.511450	0.006556	0.706449
-34.808489	-2.040232	1.516454	0.006588	0.706448
-34.843856	-2.080857	1.521459	0.006595	0.706354
-35.960900	-1.993087	1.526464	0.006803	0.706130
-35.686196	-2.039510	1.531469	0.006752	0.706135
-35.894585	-2.001773	1.536474	0.006790	0.706137
-35.862191	-2.011182	1.541478	0.006784	0.706130
-35.481975	-2.074896	1.546483	0.006713	0.706138
-35.537086	-2.067622	1.551488	0.006723	0.706133
-35.810413	-2.055569	1.556493	0.006774	0.706059
-36.634794	-2.002837	1.561498	0.006927	0.705870
-36.343029	-2.058123	1.566502	0.006873	0.705864
-36.372920	-2.049251	1.571507	0.006879	0.705871
-36.557660	-2.019687	1.576512	0.006913	0.705865
-36.464930	-2.034067	1.581517	0.006895	0.705869
-36.087047	-2.101868	1.586522	0.006825	0.705868
-36.568718	-2.128769	1.591526	0.006915	0.705642
-37.623756	-1.992562	1.596531	0.007111	0.705538
-37.440771	-2.030009	1.601536	0.007077	0.705528
-37.267114	-2.059513	1.606541	0.007044	0.705531
-37.558339	-2.005072	1.611546	0.007098	0.705537
-37.501821	-2.020561	1.616550	0.007088	0.705526
-37.181614	-2.074323	1.621555	0.007028	0.705533
-37.915563	-2.051897	1.626560	0.007165	0.705315
-38.694956	-1.960798	1.631565	0.007310	0.705219
-37.876313	-2.105961	1.636570	0.007157	0.705220
-38.301431	-2.034711	1.641574	0.007236	0.705211
-38.434489	-2.004935	1.646579	0.007261	0.705224
-37.915030	-2.102741	1.651584	0.007164	0.705214
-38.281713	-2.035161	1.656589	0.007232	0.705218
-38.894138	-2.046547	1.661594	0.007346	0.704976
-39.319158	-2.015447	1.666598	0.007425	0.704886
-38.866908	-2.092479	1.671603	0.007341	0.704893
-39.294136	-2.018911	1.676608	0.007420	0.704888
-39.480421	-1.983834	1.681613	0.007455	0.704892
-39.043550	-2.060024	1.686618	0.007373	0.704896
-39.204716	-2.034615	1.691622	0.007403	0.704889
-39.496373	-2.072132	1.696627	0.007457	0.704709
-40.222795	-2.002624	1.701632	0.007593	0.704589
-40.014818	-2.038520	1.706637	0.007554	0.704591
-40.114407	-2.018277	1.711642	0.007572	0.704596
-40.481928	-1.956279	1.716646	0.007640	0.704590
-39.892167	-2.057670	1.721651	0.007531	0.704597
-40.077390	-2.026462	1.726656	0.007565	0.704594
-40.369743	-2.043683	1.731661	0.007619	0.704454
-40.921154	-2.038555	1.736666	0.007722	0.704267
-40.924856	-2.042100	1.741670	0.007722	0.704258
-41.086334	-2.009123	1.746675	0.007752	0.704267
-40.988978	-2.028631	1.751680	0.007734	0.704263
-40.963921	-2.032891	1.756685	0.007729	0.704264
-41.131384	-2.001053	1.761690	0.007760	0.704268
-41.280261	-2.011153	1.766694	0.007788	0.704194
-41.564854	-2.076529	1.771699	0.007841	0.703960
-41.712977	-2.054754	1.776704	0.007868	0.703951
-42.268853	-1.952017	1.781709	0.007972	0.703959
-41.596461	-2.071435	1.786714	0.007847	0.703960
-41.570501	-2.080072	1.791718	0.007842	0.703952
-41.856783	-2.025082	1.796723	0.007895	0.703960
-41.951499	-2.069421	1.801728	0.007912	0.703837
-42.693880	-2.035227	1.806733	0.008050	0.703639
-42.584197	-2.052368	1.811738	0.008030	0.703644
-42.980507	-1.985576	1.816742	0.008104	0.703636
-42.832941	-2.006416	1.821747	0.008076	0.703647
-42.416131	-2.085458	1.826752	0.007998	0.703638
-42.776023	-2.022915	1.831757	0.008065	0.703635
-42.573699	-2.120715	1.836762	0.008027	0.703511
-43.807116	-1.985140	1.841766	0.008257	0.703341
-43.581341	-2.020272	1.846771	0.008215	0.703351
-43.705377	-2.001550	1.851776	0.008238	0.703345
-43.657470	-2.011043	1.856781	0.008229	0.703343
-43.762973	-1.988937	1.861786	0.008248	0.703350
-43.898111	-1.967230	1.866790	0.008273	0.703345
-43.575787	-2.060735	1.871795	0.008213	0.703273
-44.458461	-2.034707	1.876800	0.008378	0.703007
-44.728978	-1.985350	1.881805	0.008428	0.703010
-44.430439	-2.036702	1.886810	0.008372	0.703014
-44.525034	-2.022916	1.891814	0.008390	0.703008
-44.402101	-2.040993	1.896819	0.008367	0.703016
-44.537917	-2.020207	1.901824	0.008392	0.703009
-44.458821	-2.063267	1.906829	0.008377	0.702951
-45.245826	-2.046466	1.911834	0.008523	0.702702
-45.514047	-2.003619	1.916838	0.008573	0.702692
-45.377965	-2.022961	1.921843	0.008548	0.702702
-45.302284	-2.039992	1.926848	0.008534	0.702695
-45.433959	-2.016042	1.931853	0.008558	0.702696
-45.314278	-2.035048	1.936858	0.008536	0.702701
-45.448819	-2.042519	1.941862	0.008561	0.702638
-46.293605	-2.018985	1.946867	0.008718	0.702381
-46.210326	-2.036134	1.951872	0.008702	0.702376
-46.302522	-2.021036	1.956877	0.008719	0.702374
-46.141096	-2.044938	1.961882	0.008689	0.702384
-46.567984	-1.973261	1.966886	0.008768	0.702375
-46.278897	-2.021388	1.971891	0.008714	0.702382
-46.214912	-2.041736	1.976896	0.008702	0.702364
-47.119377	-2.022245	1.981901	0.008871	0.702078
-46.849211	-2.068699	1.986906	0.008820	0.702082
-47.087818	-2.032513	1.991910	0.008865	0.702069
-46.837337	-2.072642	1.996915	0.008818	0.702078
-47.215451	-2.004811	2.001920	0.008888	0.702079

-47.120538	-2.064000	2.011917	0.008870	0.701994
-47.778226	-2.068361	2.021914	0.008993	0.701749
-48.051937	-2.020348	2.031910	0.009043	0.701747
-47.913484	-2.045430	2.041907	0.009017	0.701747
-48.035565	-2.023754	2.051904	0.009040	0.701747
-48.061215	-2.018653	2.061901	0.009044	0.701749
-47.882511	-2.049599	2.071898	0.009011	0.701751
-47.989202	-1.994798	2.081894	0.009031	0.701824
-46.788682	-2.082704	2.091891	0.008807	0.702080
-47.086810	-2.030764	2.101888	0.008862	0.702077
-47.056623	-2.036815	2.111885	0.008856	0.702077
-47.170998	-2.014389	2.121882	0.008877	0.702081
-47.101532	-2.027751	2.131878	0.008864	0.702080
-47.070383	-2.034321	2.141875	0.008858	0.702078
-47.024372	-2.045047	2.151872	0.008849	0.702073
-46.873774	-2.018327	2.161869	0.008821	0.702182
-45.999736	-2.077096	2.171866	0.008658	0.702379
-46.140645	-2.052606	2.181862	0.008684	0.702378
-46.242305	-2.035422	2.191859	0.008703	0.702376
-46.457427	-1.997007	2.201856	0.008743	0.702377
-45.516336	-2.013925	2.211853	0.008567	0.702682
-45.347611	-2.034311	2.221850	0.008536	0.702702
-45.331737	-2.038545	2.231846	0.008532	0.702700
-45.421722	-2.023057	2.241843	0.008549	0.702699
-44.773771	-1.994178	2.251840	0.008428	0.702991
-44.406392	-2.051248	2.261837	0.008360	0.703009
-44.403679	-2.049848	2.271834	0.008359	0.703013
-44.424490	-2.031683	2.281830	0.008362	0.703043
-43.682157	-2.015296	2.291827	0.008224	0.703343
-43.650553	-2.019509	2.301824	0.008218	0.703347
-43.272202	-2.085031	2.311821	0.008147	0.703351
-43.657037	-1.960631	2.321818	0.008219	0.703464
-42.575614	-2.065075	2.331814	0.008017	0.703643
-42.800282	-2.027283	2.341811	0.008059	0.703639
-42.642077	-2.056619	2.351808	0.008029	0.703637
-42.056489	-2.039382	2.361805	0.007920	0.703883
-42.058665	-2.003565	2.371802	0.007920	0.703955
-41.846846	-2.041140	2.381798	0.007880	0.703955
-42.048415	-1.951530	2.391795	0.007918	0.704064
-41.077279	-2.027276	2.401792	0.007737	0.704261
-40.913397	-2.056228	2.411789	0.007706	0.704262
-41.207498	-2.002227	2.421786	0.007760	0.704265
-40.303054	-2.009645	2.431782	0.007592	0.704576
-40.161103	-2.027708	2.441779	0.007565	0.704591
-40.019787	-2.052909	2.451776	0.007539	0.704591
-40.042468	-1.997772	2.461773	0.007543	0.704695
-39.135485	-2.061479	2.471770	0.007374	0.704892
-39.259298	-2.040624	2.481766	0.007396	0.704890
-39.254995	-2.042100	2.491763	0.007395	0.704889
-38.584419	-2.035895	2.501760	0.007270	0.705143
-38.387709	-2.037323	2.511757	0.007234	0.705211
-38.366670	-2.039842	2.521754	0.007229	0.705214
-38.289607	-2.009966	2.531750	0.007215	0.705302
-37.398754	-2.056725	2.541747	0.007049	0.705528
-37.378654	-2.060862	2.551744	0.007045	0.705528
-37.584629	-2.024899	2.561741	0.007083	0.705526
-36.703915	-2.069539	2.571738	0.006919	0.705753
-36.481481	-2.053106	2.581734	0.006877	0.705866
-36.804771	-1.996663	2.591731	0.006937	0.705864
-36.610261	-2.018755	2.601728	0.006901	0.705890
-36.014072	-2.006053	2.611725	0.006789	0.706130
-35.763526	-2.049824	2.621722	0.006743	0.706132
-35.728263	-2.055226	2.631718	0.006736	0.706134
-35.100184	-2.047773	2.641715	0.006619	0.706374
-35.053335	-2.022350	2.651712	0.006610	0.706443
-34.760399	-2.073441	2.661709	0.006555	0.706445
-34.894944	-2.004992	2.671706	0.006580	0.706535
-33.834221	-2.084140	2.681702	0.006382	0.706756
-34.018090	-2.052471	2.691699	0.006416	0.706755
-33.877632	-2.077903	2.701696	0.006390	0.706754
-33.570764	-2.013673	2.711693	0.006332	0.706994
-33.070282	-2.057310	2.721690	0.006239	0.707085
-32.877080	-2.091674	2.731686	0.006203	0.707086
-33.073560	-2.040168	2.741683	0.006239	0.707120
-32.483744	-2.017850	2.751680	0.006129	0.707376
-32.240650	-2.061144	2.761677	0.006084	0.707376
-32.388800	-2.032611	2.771674	0.006111	0.707381
-31.603900	-2.038425	2.781670	0.005965	0.707650
-31.608691	-2.012147	2.791667	0.005965	0.707702
-31.247728	-2.075821	2.801664	0.005898	0.707704
-31.368244	-1.995533	2.811661	0.005920	0.707822
-30.372494	-2.075774	2.821658	0.005734	0.708017
-30.626625	-2.031122	2.831654	0.005782	0.708016
-30.518098	-2.050667	2.841651	0.005761	0.708016
-30.083646	-1.975067	2.851648	0.005680	0.708324
-29.649463	-2.037789	2.861645	0.005599	0.708353
-29.501994	-2.063454	2.871642	0.005571	0.708355
-29.347227	-2.018399	2.881638	0.005542	0.708501
-28.745511	-2.055039	2.891635	0.005430	0.708643
-28.841054	-2.037517	2.901632	0.005448	0.708644
-29.083486	-1.985082	2.911629	0.005492	0.708663
-28.073142	-2.016441	2.921626	0.005304	0.708961
-28.041223	-2.020851	2.931622	0.005298	0.708964
-28.107530	-2.010879	2.941619	0.005310	0.708961
-27.522141	-1.998576	2.951616	0.005201	0.709195
-27.434761	-1.977654	2.961613	0.005184	0.709269
-26.973553	-2.059220	2.971610	0.005098	0.709270
-27.098050	-1.972270	2.981606	0.005121	0.709400
-26.176108	-2.037941	2.991603	0.004949	0.709598
-26.261195	-2.023064	3.001600	0.004965	0.709598
-26.374431	-2.001022	3.011597	0.004986	0.709602
-25.344051	-2.047650	3.021594	0.004794	0.709876
-25.529207	-2.004196	3.031590	0.004828	0.709898
-25.269539	-2.051802	3.041587	0.004780	0.709895
-25.326243	-1.990317	3.051584	0.004790	0.709999
-24.571610	-2.014002	3.061581	0.004649	0.710220
-24.429396	-2.037318	3.071578	0.004622	0.710225
-24.660842	-1.996677	3.081574	0.004665	0.710224
-23.716630	-2.012485	3.091571	0.004489	0.710529
-23.804878	-1.992782	3.101568	0.004506	0.710537
-23.582450	-2.031718	3.111565	0.004464	0.710539
-23.255131	-2.009889	3.121562	0.004403	0.710700
-22.582356	-2.040746	3.131558	0.004277	0.710878
-22.803475	-2.002416	3.141555	0.004318	0.710876
-22.833403	-1.997758	3.151552	0.004324	0.710875
-22.037096	-2.019517	3.161549	0.004175	0.711116
-21.994215	-2.012642	3.171546	0.004167	0.711145
-21.993537	-2.012537	3.181542	0.004167	0.711146
-21.581611	-2.003555	3.191539	0.004090	0.711311
-21.263775	-1.986248	3.201536	0.004030	0.711459
-21.152806	-2.005793	3.211533	0.004009	0.711459
-21.041271	-1.998137	3.221530	0.003988	0.711515
-20.343129	-1.994254	3.231526	0.003858	0.711771
-19.942906	-2.067877	3.241523	0.003783	0.711767
-20.217866	-2.018940	3.251520	0.003834	0.711767
-19.789395	-1.992875	3.261517	0.003754	0.711972
-19.435643	-1.992987	3.271514	0.003688	0.712097
-19.297376	-2.018688	3.281510	0.003662	0.712096
-19.224702	-2.007375	3.291507	0.003649	0.712145
-18.746438	-1.969099	3.301504	0.003559	0.712391
-18.312485	-2.046181	3.311501	0.003478	0.712392
-18.372846	-2.035240	3.321498	0.003489	0.712393
-17.894108	-2.008262	3.331494	0.003400	0.712617
-17.654341	-2.002957	3.341491	0.003355	0.712713
-17.718667	-1.990879	3.351488	0.003367	0.712714
-17.540998	-1.973838	3.361485	0.003334	0.712812
-16.594340	-2.033677	3.371482	0.003157	0.713029
-16.785452	-2.000348	3.381478	0.003192	0.713028
-16.794757	-1.998974	3.391475	0.003194	0.713028
-15.993623	-1.994718	3.401472	0.003045	0.713321
-15.555675	-2.052749	3.411469	0.002963	0.713361
-15.766472	-2.013715	3.421466	0.003002	0.713364
-15.782299	-1.987965	3.431462	0.003005	0.713410
-15.010558	-2.002947	3.441459	0.002861	0.713654
-14.969866	-2.011658	3.451456	0.002853	0.713652
-15.144552	-1.979685	3.461453	0.002885	0.713654
-14.241825	-2.009817	3.471450	0.002717	0.713914
-14.112680	-2.001223	3.481446	0.002693	0.713977
-14.076676	-2.010947	3.491443	0.002686	0.713971
-13.949613	-1.990499	3.501440	0.002662	0.714057
-12.941310	-2.056856	3.511437	0.002474	0.714283
-13.157497	-2.018160	3.521434	0.002514	0.714283
-12.899969	-2.063647	3.531430	0.002466	0.714285
-12.998722	-1.949690	3.541427	0.002484	0.714476
-12.277861	-2.009715	3.551424	0.002350	0.714613
-12.514798	-1.968031	3.561421	0.002393	0.714612
-12.173178	-1.985011	3.571418	0.002330	0.714699
-11.389437	-2.014641	3.581414	0.002183	0.714918
-11.605314	-1.979741	3.591411	0.002223	0.714912
-11.491081	-2.001001	3.601408	0.002202	0.714910
-10.742287	-1.998260	3.611405	0.002062	0.715181
-10.803819	-1.959818	3.621402	0.002074	0.715236
-10.207399	-2.063614	3.631398	0.001962	0.715241
-10.459418	-1.987736	3.641395	0.002009	0.715303
-9.220688	-2.083562	3.651392	0.001778	0.715551
-9.391023	-2.053193	3.661389	0.001810	0.715551
-9.245604	-2.078707	3.671386	0.001782	0.715552
-9.207704	-2.057684	3.681382	0.001775	0.715608
-8.280160	-2.081782	3.691379	0.001602	0.715888
-8.018368	-2.129126	3.701376	0.001553	0.715887
-8.158228	-2.104264	3.711373	0.001579	0.715887
-8.380833	-2.063285	3.721370	0.001620	0.715890
-7.435183	-2.112553	3.731366	0.001444	0.716127
-7.588584	-2.078417	3.741363	0.001472	0.716141
-7.293219	-2.132647	3.751360	0.001417	0.716138
-7.644062	-2.032030	3.761357	0.001482	0.716214
-6.333367	-2.143845	3.771354	0.001238	0.716455
-6.553734	-2.105829	3.781350	0.001279	0.716453
-6.765358	-2.068226	3.791347	0.001318	0.716454
-6.295674	-2.057765	3.801344	0.001230	0.716640
-5.673492	-2.108977	3.811341	0.001114	0.716759
-5.658815	-2.109428	3.821338	0.001111	0.716763
-5.520126	-2.134214	3.831334	0.001085	0.716764
-4.866144	-2.087382	3.841331	0.000963	0.717087
-4.798209	-2.097039	3.851328	0.000950	0.717093
-4.817678	-2.096581	3.861325	0.000954	0.717087
-4.728899	-2.048137	3.871322	0.000937	0.717215
-3.655567	-2.151032	3.881318	0.000737	0.717389
-3.853877	-2.117541	3.891315	0.000774	0.717386
-3.629470	-2.158145	3.901312	0.000732	0.717385
-3.423830	-2.087049	3.911309	0.000693	0.717599
-2.764742	-2.147904	3.921306	0.000570	0.717711
-2.866405	-2.130875	3.931302	0.000589	0.717709
-2.812380	-2.140226	3.941299	0.000579	0.717710
-2.419494	-2.062246	3.951296	0.000505	0.718003
-1.880203	-2.148599	3.961293	0.000405	0.718023
-2.246268	-2.083498	3.971290	0.000473	0.718023
-2.075434	-2.021966	3.981286	0.000441	0.718205
-1.247233	-2.090210	3.991283	0.000286	0.718362
-1.654694	-2.019756	4.001280	0.000362	0.718358
-1.415148	-2.010583	4.011277	0.000317	0.718461
-1.160907	-1.960678	4.021274	0.000269	0.718649
-1.356351	-1.926833	4.031270	0.000306	0.718648
-1.218991	-1.839934	4.041267	0.000280	0.718868
-1.400866	-1.758692	4.051264	0.000313	0.718965
-0.932409	-1.767419	4.061261	0.000226	0.719113
-0.996358	-1.673841	4.071258	0.000238	0.719275
-1.035306	-1.596386	4.081254	0.000245	0.719415
-0.831854	-1.535959	4.091251	0.000206	0.719606
-0.748917	-1.470064	4.101248	0.000191	0.719765
-0.685270	-1.410392	4.111245	0.000179	0.719905
-0.609171	-1.293228	4.121242	0.000164	0.720163
-0.583577	-1.232414	4.131238	0.000159	0.720293
-0.339372	-1.146856	4.141235	0.000113	0.720547
-0.623858	-0.989434	4.151232	0.000166	0.720758
-0.331769	-0.952227	4.161229	0.000111	0.720934
-0.524181	-0.819562	4.171226	0.000147	0.721128
-0.254376	-0.728952	4.181222	0.000096	0.721401
-0.135135	-0.645587	4.191219	0.000074	0.721607
0.067341	-0.568342	4.201216	0.000036	0.721830
0.156226	-0.457316	4.211213	0.000019	0.722080
0.097827	-0.298262	4.221210	0.000030	0.722372
0.020278	-0.152018	4.231206	0.000044	0.722633
-0.059610	0.002692	4.241203	0.000058	0.722909
0.000000	0.166347	4.251200	0.000047	0.723251

-0.019370	0.828518	4.256205	0.000050	0.724542
0.219607	2.047067	4.261210	0.000005	0.727008
0.417869	3.875452	4.266214	-0.000034	0.730636
0.893878	6.211015	4.271219	-0.000124	0.735321
1.048838	9.105857	4.276224	-0.000155	0.740938
1.398369	12.455676	4.281229	-0.000222	0.747443
2.061270	16.200484	4.286234	-0.000348	0.754739
2.146725	20.452441	4.291238	-0.000367	0.762718
2.660401	25.034605	4.296243	-0.000466	0.771362
3.221908	29.963203	4.301248	-0.000573	0.780556
3.774126	35.256892	4.306253	-0.000680	0.790294
4.069850	40.907296	4.311258	-0.000739	0.800466
4.494592	46.835995	4.316262	-0.000822	0.811037
4.946896	53.042995	4.321267	-0.000910	0.821960
5.320208	59.535841	4.326272	-0.000984	0.833203
5.946282	66.201585	4.331277	-0.001105	0.844661
6.592269	73.094813	4.336282	-0.001230	0.856349
9.290527	79.840981	4.341286	-0.001737	0.868228
10.200639	87.129015	4.346291	-0.001911	0.880313
10.796039	94.634705	4.351296	-0.002027	0.892491
12.051076	102.201571	4.356301	-0.002266	0.904782
12.964665	109.982177	4.361306	-0.002441	0.917146
13.740195	117.894689	4.366310	-0.002591	0.929509
14.488214	125.928962	4.371315	-0.002735	0.941885
15.311434	134.048433	4.376320	-0.002894	0.954247
16.127875	142.247707	4.381325	-0.003051	0.966566
17.099790	150.510580	4.386330	-0.003238	0.978860
18.139325	158.845818	4.391334	-0.003437	0.991121
19.058955	167.261980	4.396339	-0.003614	1.003317
19.851119	175.733857	4.401344	-0.003767	1.015413
20.505744	184.270397	4.406349	-0.003895	1.027423
21.143559	192.848456	4.411354	-0.004019	1.039346
22.237316	201.362810	4.416358	-0.004228	1.051153
23.119418	209.953685	4.421363	-0.004398	1.062882
23.719229	218.615934	4.426368	-0.004516	1.074513
24.460817	227.246940	4.431373	-0.004659	1.086010
25.180606	235.896835	4.436378	-0.004799	1.097405
25.743432	244.576642	4.441382	-0.004910	1.108687
26.816437	253.184618	4.446387	-0.005115	1.119875
27.585763	261.825790	4.451392	-0.005264	1.130927
28.138737	270.507867	4.456397	-0.005373	1.141877
28.760343	279.199434	4.461402	-0.005495	1.152749
29.333187	287.839884	4.466406	-0.005607	1.163447
30.230498	296.430430	4.471411	-0.005780	1.174053
30.723695	305.061808	4.476416	-0.005877	1.184531
31.525183	313.659667	4.481421	-0.006032	1.194938
32.660711	322.167395	4.486426	-0.006249	1.205217
33.372705	330.759835	4.491430	-0.006388	1.215422
34.155703	339.325961	4.496435	-0.006539	1.225526
34.497703	347.962828	4.501440	-0.006609	1.235542
35.416902	356.453498	4.506445	-0.006785	1.245423
36.080319	364.996115	4.511450	-0.006915	1.255235
36.808476	373.500937	4.516454	-0.007056	1.264940
37.642024	382.000582	4.521459	-0.007217	1.274585
38.301466	390.491586	4.526464	-0.007345	1.284115
38.911552	399.006180	4.531469	-0.007464	1.293592
39.694399	407.458305	4.536474	-0.007616	1.302963
40.155614	416.043952	4.541478	-0.007707	1.312353
40.786780	424.526852	4.546483	-0.007830	1.321596
41.319286	432.947794	4.551488	-0.007935	1.330691
42.034194	441.340261	4.556493	-0.008074	1.339726
42.262078	449.804705	4.561498	-0.008122	1.348691
42.800122	458.200685	4.566502	-0.008228	1.357578
43.612691	466.535738	4.571507	-0.008385	1.366392
44.210902	474.913280	4.576512	-0.008501	1.375156
44.745805	483.298936	4.581517	-0.008607	1.383862
45.469606	491.660650	4.586522	-0.008747	1.392521
45.999152	500.009756	4.591526	-0.008851	1.401080
46.529311	508.370631	4.596531	-0.008955	1.409600
47.036529	516.715199	4.601536	-0.009055	1.418048
47.801560	525.005884	4.606541	-0.009203	1.426434
48.347703	533.353844	4.611546	-0.009311	1.434792
48.922339	541.652532	4.616550	-0.009423	1.443057
49.644867	549.956975	4.621555	-0.009563	1.451305
50.235077	558.257984	4.626560	-0.009679	1.459481
50.707471	566.585329	4.631565	-0.009772	1.467618
51.335192	574.934489	4.636570	-0.009894	1.475756
51.578821	583.234277	4.641574	-0.009945	1.483741
52.092835	591.529900	4.646579	-0.010047	1.491722
52.422883	599.819268	4.651584	-0.010114	1.499625
53.036004	608.061051	4.656589	-0.010233	1.507486
53.693754	616.329925	4.661594	-0.010361	1.515338
54.132325	624.578214	4.666598	-0.010448	1.523097
54.668213	632.839716	4.671603	-0.010554	1.530843
55.308308	641.070107	4.676608	-0.010678	1.538537
55.790098	649.329354	4.681613	-0.010773	1.546195
56.158667	657.619935	4.686618	-0.010848	1.553827
56.538087	665.848017	4.691622	-0.010924	1.561367
57.232149	674.057656	4.696627	-0.011058	1.568899
57.525076	682.321056	4.701632	-0.011118	1.576386
58.113296	690.528092	4.706637	-0.011233	1.583829
58.707623	698.748251	4.711642	-0.011350	1.591249
58.988572	707.006772	4.716646	-0.011407	1.598625
59.493924	715.201461	4.721651	-0.011507	1.605941
59.955602	723.428176	4.726656	-0.011598	1.613247
60.533281	731.619203	4.731661	-0.011711	1.620504
61.032270	739.829556	4.736666	-0.011810	1.627735
61.391491	748.103658	4.741670	-0.011882	1.634969
61.886422	756.283569	4.746675	-0.011980	1.642109
62.145393	764.496524	4.751680	-0.012033	1.649213
62.686154	772.679260	4.756685	-0.012139	1.656300
63.182609	780.857787	4.761690	-0.012237	1.663347
63.564241	789.053709	4.766694	-0.012314	1.670363
64.269882	797.226950	4.771699	-0.012451	1.677373
64.812187	805.376561	4.776704	-0.012557	1.684313
65.440640	813.553878	4.781709	-0.012680	1.691259
65.569552	821.799788	4.786714	-0.012709	1.698167
66.121383	829.941035	4.791718	-0.012817	1.705016
66.538315	838.164033	4.796723	-0.012900	1.711888
66.905192	846.335404	4.801728	-0.012974	1.718682
67.188558	854.492924	4.806733	-0.013032	1.725428
67.721973	862.661828	4.811738	-0.013137	1.732189
68.143901	870.819544	4.816742	-0.013221	1.738900
68.804709	878.948030	4.821747	-0.013349	1.745591
69.411309	887.094663	4.826752	-0.013468	1.752265
69.775198	895.283130	4.831757	-0.013541	1.758916
70.028504	903.453078	4.836762	-0.013594	1.765513
70.471088	911.613099	4.841766	-0.013681	1.772102
70.891724	919.791685	4.846771	-0.013765	1.778678
71.516579	927.896882	4.851776	-0.013887	1.785196
71.986086	936.092957	4.856781	-0.013980	1.791743
72.571666	944.249605	4.861786	-0.014094	1.798250
73.103322	952.352219	4.866790	-0.014199	1.804684
73.433320	960.530591	4.871795	-0.014266	1.811129
74.040150	968.637465	4.876800	-0.014384	1.817530
74.404428	976.793573	4.881805	-0.014457	1.823916
74.883963	984.937316	4.886810	-0.014552	1.830285
75.468281	993.057573	4.891814	-0.014666	1.836626
75.850706	1001.214269	4.896819	-0.014743	1.842949
76.002682	1009.386139	4.901824	-0.014776	1.849234
76.457373	1017.532112	4.906829	-0.014866	1.855514
76.989428	1025.646282	4.911834	-0.014971	1.861757
77.321013	1033.794078	4.916838	-0.015038	1.867982
77.854783	1041.960688	4.921843	-0.015143	1.874223
78.287810	1050.057376	4.926848	-0.015229	1.880380
78.753889	1058.158937	4.931853	-0.015321	1.886523
79.274440	1066.294320	4.936858	-0.015423	1.892678
79.666720	1074.432784	4.941862	-0.015502	1.898801
80.292210	1082.519327	4.946867	-0.015624	1.904891
80.576339	1090.673820	4.951872	-0.015682	1.910974
80.684925	1098.858881	4.956877	-0.015708	1.917041
81.307331	1106.924246	4.961882	-0.015829	1.923057
81.489905	1115.076346	4.966886	-0.015868	1.929069
81.840412	1123.227744	4.971891	-0.015939	1.935081
82.104649	1131.334091	4.976896	-0.015994	1.941031
82.604926	1139.436607	4.981901	-0.016092	1.946986
82.923921	1147.613071	4.986906	-0.016157	1.952957
83.078794	1155.745229	4.991910	-0.016191	1.958860
83.492077	1163.826208	4.996915	-0.016274	1.964736
83.566331	1171.952777	5.001920	-0.016293	1.970591
83.996002	1180.044546	5.006925	-0.016378	1.976441
84.421739	1188.145085	5.011930	-0.016463	1.982280
85.024068	1196.198268	5.016934	-0.016580	1.988086
85.353378	1204.341096	5.021939	-0.016647	1.993910
85.539485	1212.458465	5.026944	-0.016687	1.999685
86.240212	1220.490142	5.031949	-0.016823	2.005435
86.664382	1228.613623	5.036954	-0.016907	2.011205
86.980586	1236.734033	5.041958	-0.016972	2.016945
87.703035	1244.798351	5.046963	-0.017112	2.022671
87.865101	1252.948707	5.051968	-0.017147	2.028384
88.322943	1261.088811	5.056973	-0.017238	2.034103
88.791293	1269.164743	5.061978	-0.017330	2.039763
88.978188	1277.268444	5.066982	-0.017371	2.045397
89.376725	1285.380191	5.071987	-0.017450	2.051043
89.861641	1293.472060	5.076992	-0.017546	2.056669
90.358262	1301.550893	5.081997	-0.017644	2.062271
90.684556	1309.658924	5.087002	-0.017710	2.067861
90.920545	1317.781969	5.092006	-0.017759	2.073437
91.337433	1325.886566	5.097011	-0.017842	2.079003
91.668630	1333.959919	5.102016	-0.017909	2.084524
92.103520	1342.042686	5.107021	-0.017996	2.090048
92.684989	1350.134982	5.112026	-0.018109	2.095577
93.035833	1358.206927	5.117030	-0.018180	2.101056
93.362962	1366.325496	5.122035	-0.018246	2.106549
93.622516	1374.480400	5.127040	-0.018300	2.112046
94.069840	1382.583014	5.132045	-0.018389	2.117512
94.525786	1390.624898	5.137050	-0.018479	2.122923
94.649068	1398.725818	5.142054	-0.018507	2.128329
95.064564	1406.827659	5.147059	-0.018590	2.133749
95.225230	1414.919447	5.152064	-0.018625	2.139124
95.703885	1422.968505	5.157069	-0.018720	2.144487
96.135335	1431.055507	5.162074	-0.018805	2.149858
96.388161	1439.162162	5.167078	-0.018858	2.155211
96.853182	1447.232740	5.172083	-0.018950	2.160548
97.176339	1455.299853	5.177088	-0.019015	2.165855
97.773822	1463.364093	5.182093	-0.019132	2.171173
98.154260	1471.476471	5.187098	-0.019208	2.176489
98.521920	1479.538106	5.192102	-0.019282	2.181758
98.981412	1487.629688	5.197107	-0.019373	2.187041
99.286932	1495.745045	5.202112	-0.019435	2.192314
99.691166	1503.819468	5.207117	-0.019516	2.197556
99.939717	1511.901388	5.212122	-0.019568	2.202776
100.227724	1519.979346	5.217126	-0.019627	2.207985
100.661652	1528.076620	5.222131	-0.019713	2.213207
100.899810	1536.160111	5.227136	-0.019763	2.218390
101.291083	1544.217702	5.232141	-0.019841	2.223559
101.382674	1552.338461	5.237146	-0.019863	2.228728
101.746457	1560.417224	5.242150	-0.019936	2.233884
102.180247	1568.482931	5.247155	-0.020022	2.239025
102.667282	1576.521710	5.252160	-0.020118	2.244142
103.102568	1584.592350	5.257165	-0.020205	2.249263
103.620596	1592.673949	5.262170	-0.020307	2.254386
103.918967	1600.747187	5.267174	-0.020368	2.259473
104.126619	1608.856154	5.272179	-0.020412	2.264563
104.414077	1616.937182	5.277184	-0.020471	2.269630
104.858228	1625.087388	5.282189	-0.020559	2.274744
105.391808	1633.095270	5.287194	-0.020663	2.279764
105.425045	1641.166630	5.292198	-0.020675	2.284771
105.906347	1649.224702	5.297203	-0.020770	2.289796
106.094311	1657.327928	5.302208	-0.020810	2.294813
106.494230	1665.357297	5.307213	-0.020890	2.299791
107.103552	1673.396037	5.312218	-0.021009	2.304782
107.323418	1681.473502	5.317222	-0.021055	2.309754
107.852467	1689.564902	5.322227	-0.021159	2.314748
108.276800	1697.608312	5.327232	-0.021243	2.319694
108.649207	1705.659073	5.332237	-0.021318	2.324630
108.883823	1713.760845	5.337242	-0.021367	2.329574
109.061335	1721.864053	5.342246	-0.021406	2.334504
109.393303	1729.937781	5.347251	-0.021473	2.339419
109.576294	1738.004386	5.352256	-0.021512	2.344306
109.954158	1746.072004	5.357261	-0.021588	2.349200
110.563820	1754.155578	5.362266	-0.021707	2.354112
110.597027	1762.228163	5.367270	-0.021718	2.358961
110.932225	1770.285117	5.372275	-0.021786	2.363814
111.308040	1778.324137	5.377280	-0.021862	2.368650
111.816613	1786.382475	5.382285	-0.021962	2.373498
112.217830	1794.439473	5.387290	-0.022042	2.378327
112.571183	1802.481655	5.392294	-0.022113	2.383133
112.873724	1810.579781	5.397299	-0.022175	2.387959
113.069256	1818.693453	5.402304	-0.022216	2.392776
113.481768	1826.723289	5.407309	-0.022299	2.397550
113.847122	1834.790796	5.412314	-0.022372	2.402334
114.167413	1842.843956	5.417318	-0.022437	2.407095
114.534215	1850.935603	5.422323	-0.022511	2.411874
114.879729	1858.994092	5.427328	-0.022580	2.416622
115.124708	1867.048547	5.432333	-0.022631	2.421350
115.533219	1875.121172	5.437338	-0.022713	2.426093
115.666939	1883.219244	5.442342	-0.022743	2.430819
115.856035	1891.367826	5.447347	-0.022784	2.435570
116.284259	1899.362071	5.452352	-0.022869	2.440241
116.537755	1907.363531	5.457357	-0.022921	2.444893
116.819954	1915.439102	5.462362	-0.022979	2.449582
116.853888	1923.528397	5.467366	-0.022991	2.454250
117.409738	1931.545176	5.472371	-0.023100	2.458908
117.450772	1939.612004	5.477376	-0.023113	2.463546
117.959729	1947.639159	5.482381	-0.023213	2.468188
118.294036	1955.718654	5.487386	-0.023280	2.472838
118.610655	1963.757905	5.492390	-0.023345	2.477455
118.926787	1971.809140	5.497395	-0.023409	2.482070
119.356328	1979.857606	5.502400	-0.023494	2.486684
119.781302	1987.927391	5.507405	-0.023579	2.491300
119.862731	1996.032491	5.512410	-0.023599	2.495902
120.113445	2004.068987	5.517414	-0.023651	2.500470
120.643464	2012.092727	5.522419	-0.023755	2.505042
120.508797	2020.208775	5.527424	-0.023736	2.509610
121.086904	2028.288684	5.532429	-0.023849	2.514201
121.570462	2036.304642	5.537434	-0.023944	2.518740
121.601512	2044.357269	5.542438	-0.023955	2.523259
122.084115	2052.391579	5.547443	-0.024050	2.527793
122.249043	2060.476623	5.552448	-0.024086	2.532323
122.723783	2068.504365	5.557453	-0.024180	2.536836
123.127086	2076.564195	5.562458	-0.024261	2.541353
123.268044	2084.600227	5.567462	-0.024292	2.545830
123.679531	2092.668336	5.572467	-0.024374	2.550337
124.039562	2100.726179	5.577472	-0.024447	2.554826
124.243752	2108.787581	5.582477	-0.024490	2.559298
124.673442	2116.823481	5.587482	-0.024575	2.563764
125.017415	2124.873111	5.592486	-0.024645	2.568223
125.347775	2132.953716	5.597491	-0.024712	2.572691
125.276110	2141.048646	5.602496	-0.024704	2.577132
125.801819	2149.057899	5.607501	-0.024807	2.581558
126.199952	2157.108886	5.612506	-0.024886	2.585991
126.354306	2165.183495	5.617510	-0.024920	2.590413
126.777126	2173.430776	5.622515	-0.025005	2.594939
127.109766	2181.391425	5.627520	-0.025072	2.599296
127.529147	2189.378433	5.632525	-0.025155	2.603665
127.761674	2197.427924	5.637530	-0.025204	2.608048
128.039564	2205.458087	5.642534	-0.025261	2.612417
128.374474	2213.492506	5.647539	-0.025329	2.616784
128.588815	2221.550521	5.652544	-0.025374	2.621148
128.615947	2229.599668	5.657549	-0.025384	2.625488
129.076368	2237.631776	5.662554	-0.025475	2.629840
129.191348	2245.701885	5.667558	-0.025502	2.634183
129.669578	2253.709659	5.672563	-0.025597	2.638509
129.850976	2261.748253	5.677568	-0.025636	2.642824
129.889535	2269.822538	5.682573	-0.025648	2.647143
130.535740	2277.839960	5.687578	-0.025774	2.651463
130.980066	2285.889593	5.692582	-0.025862	2.655781
131.140720	2293.960679	5.697587	-0.025897	2.660084
131.536541	2301.987539	5.702592	-0.025976	2.664372
131.826148	2310.031026	5.707597	-0.026036	2.668655
132.344197	2318.117804	5.712602	-0.026137	2.672969
132.798781	2326.141083	5.717606	-0.026227	2.677238
132.887105	2334.199737	5.722611	-0.026249	2.681495
133.223293	2342.239614	5.727616	-0.026317	2.685752
133.530958	2350.269742	5.732621	-0.026380	2.689995
133.784645	2358.377533	5.737626	-0.026432	2.694268
133.837504	2366.408006	5.742630	-0.026448	2.698481
134.228643	2374.432662	5.747635	-0.026526	2.702706
134.580228	2382.482012	5.752640	-0.026597	2.706935
134.951308	2390.519082	5.757645	-0.026671	2.711152
135.221032	2398.599554	5.762650	-0.026727	2.715379
135.612679	2406.598997	5.767654	-0.026805	2.719564
136.256481	2414.595498	5.772659	-0.026930	2.723757
136.458557	2422.673325	5.777664	-0.026973	2.727958
136.624342	2430.745696	5.782669	-0.027009	2.732148
136.796013	2438.854042	5.787674	-0.027047	2.736350
137.257953	2446.845091	5.792678	-0.027138	2.740503
137.471192	2454.896001	5.797683	-0.027183	2.744665
137.633689	2462.975549	5.802688	-0.027219	2.748833
137.904019	2471.062712	5.807693	-0.027274	2.753004
138.219288	2479.132072	5.812698	-0.027339	2.757163
138.332085	2487.130137	5.817702	-0.027365	2.761267
138.799262	2495.136670	5.822707	-0.027457	2.765390
139.138602	2503.173997	5.827712	-0.027526	2.769515
139.385303	2511.223259	5.832717	-0.027577	2.773635
139.663206	2519.276104	5.837722	-0.027634	2.777752
139.842313	2527.310732	5.842726	-0.027673	2.781848
140.224467	2535.335037	5.847731	-0.027749	2.785944
140.266772	2543.402023	5.852736	-0.027762	2.790036
140.608199	2551.456867	5.857741	-0.027831	2.794133
141.188473	2559.475211	5.862746	-0.027945	2.798220
141.170295	2567.516850	5.867750	-0.027947	2.802278
141.415928	2575.556600	5.872755	-0.027998	2.806344
141.810163	2583.579954	5.877760	-0.028077	2.810404
141.841099	2591.680322	5.882765	-0.028088	2.814477
142.099205	2599.726660	5.887770	-0.028141	2.818529
142.384135	2607.721815	5.892774	-0.028200	2.822551
142.610803	2615.779504	5.897779	-0.028247	2.826596
142.942454	2623.809429	5.902784	-0.028314	2.830627
143.188954	2631.900726	5.907789	-0.028365	2.834678
143.453768	2639.917010	5.912794	-0.028420	2.838686
143.689595	2647.929216	5.917798	-0.028469	2.842685
144.056243	2655.956323	5.922803	-0.028543	2.846694
144.333606	2664.010047	5.927808	-0.028600	2.850705
144.421340	2672.072628	5.932813	-0.028622	2.854704
144.798254	2680.112224	5.937818	-0.028697	2.858702
145.026810	2688.105916	5.942822	-0.028745	2.862663
145.303966	2696.181376	5.947827	-0.028802	2.866662
145.516423	2704.227297	5.952832	-0.028847	2.870637
145.718458	2712.260888	5.957837	-0.028890	2.874600
146.132474	2720.310087	5.962842	-0.028972	2.878577
146.221795	2728.338563	5.967846	-0.028994	2.882521
146.676827	2736.371990	5.972851	-0.029084	2.886481
146.937702	2744.420947	5.977856	-0.029138	2.890433
146.997441	2752.491775	5.982861	-0.029155	2.894379
147.403577	2760.513054	5.987866	-0.029236	2.898314
147.644607	2768.524520	5.992870	-0.029286	2.902231
147.936263	2776.581194	5.997875	-0.029346	2.906166
148.138619	2784.627886	6.002880	-0.029389	2.910087
148.332015	2792.741898	6.007885	-0.029430	2.914034
148.737679	2800.763243	6.012890	-0.029511	2.917943
148.909525	2808.746831	6.017894	-0.029548	2.921815
149.062298	2816.805244	6.022899	-0.029582	2.925718
149.442992	2824.794069	6.027904	-0.029658	2.929593
149.785221	2832.840637	6.032909	-0.029727	2.933490
150.132628	2840.885853	6.037914	-0.029797	2.937380
150.265349	2848.913791	6.042918	-0.029827	2.941246
150.532628	2856.959329	6.047923	-0.029883	2.945122
150.784629	2865.002276	6.052928	-0.029935	2.948992
151.218410	2873.037040	6.057933	-0.030021	2.952861
151.562756	2881.100020	6.062938	-0.030090	2.956734
151.726540	2889.096282	6.067942	-0.030126	2.960561
152.126288	2897.116407	6.072947	-0.030206	2.964406
152.217197	2905.185368	6.077952	-0.030228	2.968254
152.568202	2913.216795	6.082957	-0.030299	2.972093
152.647209	2921.302839	6.087962	-0.030319	2.975938
152.921748	2929.283825	6.092966	-0.030375	2.979738
153.175525	2937.347238	6.097971	-0.030428	2.983572
153.344882	2945.394441	6.102976	-0.030465	2.987388
153.487215	2953.441664	6.107981	-0.030497	2.991199
154.015296	2961.480442	6.112986	-0.030601	2.995020
154.302480	2969.456357	6.117990	-0.030659	2.998794
154.423206	2977.513027	6.122995	-0.030687	3.002593
154.655291	2985.546385	6.128000	-0.030736	3.006382
155.056447	2993.531089	6.133005	-0.030816	3.010151
155.229624	3001.628402	6.138010	-0.030853	3.013958
155.357092	3009.667452	6.143014	-0.030882	3.017730
155.769015	3017.685730	6.148019	-0.030964	3.021501
155.990255	3025.703947	6.153024	-0.031011	3.025258
156.006399	3033.756173	6.158029	-0.031019	3.029017
156.546174	3041.825956	6.163034	-0.031125	3.032804
156.620356	3049.875632	6.168038	-0.031144	3.036555
156.959801	3057.871711	6.173043	-0.031213	3.040289
157.267965	3065.883036	6.178048	-0.031276	3.044024
157.342033	3073.939157	6.183053	-0.031295	3.047764
157.676659	3082.002149	6.188058	-0.031362	3.051514
158.034874	3090.017464	6.193062	-0.031434	3.055240
158.355864	3098.039113	6.198067	-0.031500	3.058961
158.453259	3106.088727	6.203072	-0.031523	3.062681
158.706931	3114.107232	6.208077	-0.031576	3.066389
159.119189	3122.160893	6.213082	-0.031658	3.070116
159.229152	3130.283687	6.218086	-0.031684	3.073856
159.468037	3138.293905	6.223091	-0.031733	3.077546
159.656561	3146.306686	6.228096	-0.031774	3.081230
160.001951	3154.269742	6.233101	-0.031843	3.084895
160.111677	3162.336426	6.238106	-0.031869	3.088591
160.405941	3170.359487	6.243110	-0.031929	3.092272
160.795649	3178.407355	6.248115	-0.032007	3.095963
160.984808	3186.422024	6.253120	-0.032048	3.099626
161.137230	3194.442393	6.258125	-0.032082	3.103286
161.624413	3202.504272	6.263130	-0.032178	3.106975
161.858286	3210.528244	6.268134	-0.032227	3.110631
162.145564	3218.586095	6.273139	-0.032285	3.114301
162.381055	3226.622885	6.278144	-0.032335	3.117954
162.714445	3234.623691	6.283149	-0.032402	3.121591
162.965193	3242.639378	6.288154	-0.032454	3.125227
163.115790	3250.683365	6.293158	-0.032487	3.128867
163.540177	3258.733501	6.298163	-0.032572	3.132518
163.721942	3266.776091	6.303168	-0.032611	3.136150
163.662678	3274.808610	6.308173	-0.032605	3.139763
163.918838	3282.819619	6.313178	-0.032658	3.143376
164.285409	3290.850111	6.318182	-0.032732	3.146998
164.667747	3298.896875	6.323187	-0.032808	3.150624
164.890317	3306.972771	6.328192	-0.032855	3.154251
164.993956	3314.993491	6.333197	-0.032880	3.157845
165.256254	3323.010198	6.338202	-0.032934	3.161440
165.247491	3331.015389	6.343206	-0.032938	3.165014
165.710421	3339.030539	6.348211	-0.033029	3.168608
166.119582	3347.059485	6.353216	-0.033111	3.172202
166.105482	3355.126315	6.358221	-0.033114	3.175791
166.254192	3363.159312	6.363226	-0.033147	3.179367
166.395300	3371.193718	6.368230	-0.033178	3.182940
166.880042	3379.185530	6.373235	-0.033274	3.186504
166.853822	3387.264651	6.378240	-0.033274	3.190082
167.196534	3395.274122	6.383245	-0.033343	3.193640
167.534393	3403.322850	6.388250	-0.033412	3.197211
167.716478	3411.333882	6.393254	-0.033451	3.200755
168.103752	3419.314036	6.398259	-0.033528	3.204291
168.376643	3427.384154	6.403264	-0.033584	3.207856
168.678866	3435.430828	6.408269	-0.033646	3.211409
168.744242	3443.455414	6.413274	-0.033664	3.214939
168.976842	3451.498867	6.418278	-0.033712	3.218479
169.122340	3459.555138	6.423283	-0.033745	3.222018
169.336135	3467.551957	6.428288	-0.033790	3.225530
169.679743	3475.571265	6.433293	-0.033859	3.229053
169.949732	3483.662067	6.438298	-0.033915	3.232600
170.146442	3491.704988	6.443302	-0.033957	3.236119
170.605758	3499.667391	6.448307	-0.034048	3.239610
170.716309	3507.707970	6.453312	-0.034074	3.243118
170.896996	3515.714271	6.458317	-0.034112	3.246609
171.471299	3523.720555	6.463322	-0.034225	3.250112
171.844523	3531.747664	6.468326	-0.034300	3.253613
172.206764	3539.799013	6.473331	-0.034372	3.257119
172.561110	3547.789291	6.478336	-0.034444	3.260595
172.688538	3555.821142	6.483341	-0.034473	3.264077
173.019002	3563.875761	6.488346	-0.034540	3.267572
173.173363	3571.914586	6.493350	-0.034574	3.271050
173.662225	3579.960847	6.498355	-0.034670	3.274540
174.040582	3587.999791	6.503360	-0.034746	3.278019
173.955934	3596.031716	6.508365	-0.034735	3.281474
174.179662	3604.038634	6.513370	-0.034782	3.284926
174.589892	3612.069412	6.518374	-0.034864	3.288392
174.809052	3620.112810	6.523379	-0.034910	3.291852
175.178319	3628.158714	6.528384	-0.034984	3.295315
175.359308	3636.168715	6.533389	-0.035023	3.298752
175.800528	3644.199888	6.538394	-0.035111	3.302204
175.949279	3652.209989	6.543398	-0.035144	3.305633
176.114544	3660.254835	6.548403	-0.035180	3.309073
176.570925	3668.314751	6.553408	-0.035270	3.312528
176.540410	3676.355670	6.558413	-0.035270	3.315952
176.832345	3684.359025	6.563418	-0.035330	3.319369
176.958916	3692.366126	6.568422	-0.035359	3.322777
177.074294	3700.375138	6.573427	-0.035386	3.326183
177.446640	3708.409818	6.578432	-0.035460	3.329605
177.616082	3716.447721	6.583437	-0.035497	3.333018
177.779473	3724.507757	6.588442	-0.035533	3.336436
177.905210	3732.502587	6.593446	-0.035562	3.339822
178.197072	3740.534152	6.598451	-0.035621	3.343226
178.590365	3748.549780	6.603456	-0.035700	3.346623
178.681730	3756.589298	6.608461	-0.035722	3.350016
178.889420	3764.642629	6.613466	-0.035766	3.353416
179.092195	3772.670510	6.618470	-0.035809	3.356801
179.364764	3780.675383	6.623475	-0.035865	3.360175
179.558435	3788.699616	6.628480	-0.035907	3.363552
179.706353	3796.738128	6.633485	-0.035940	3.366929
180.075668	3804.777970	6.638490	-0.036014	3.370311
180.258532	3812.843315	6.643494	-0.036053	3.373694
180.372288	3820.874129	6.648499	-0.036080	3.377057
180.606414	3828.878216	6.653504	-0.036129	3.380410
180.788689	3836.883492	6.658509	-0.036168	3.383757
180.964807	3844.934011	6.663514	-0.036206	3.387120
181.325373	3852.905987	6.668518	-0.036279	3.390454
181.525821	3861.052446	6.673523	-0.036321	3.393851
181.665330	3869.101785	6.678528	-0.036353	3.397202
182.072075	3877.012898	6.683533	-0.036434	3.400502
182.426577	3885.029564	6.688538	-0.036505	3.403840
182.532791	3893.052154	6.693542	-0.036530	3.407169
182.521923	3901.067393	6.698547	-0.036533	3.410488
182.998879	3909.131929	6.703552	-0.036628	3.413840
183.121460	3917.145227	6.708557	-0.036656	3.417156
183.448473	3925.171607	6.713562	-0.036722	3.420481
183.411283	3933.184913	6.718566	-0.036720	3.423785
183.773870	3941.200724	6.723571	-0.036793	3.427100
184.111362	3949.231064	6.728576	-0.036861	3.430417
184.122823	3957.285098	6.733581	-0.036869	3.433730
184.375274	3965.341910	6.738586	-0.036921	3.437049
184.613283	3973.329419	6.743590	-0.036971	3.440335
184.852709	3981.316193	6.748595	-0.037021	3.443618
185.080501	3989.408469	6.753600	-0.037068	3.446941
185.443394	3997.381865	6.758605	-0.037141	3.450216
185.902554	4005.452353	6.763610	-0.037232	3.453531
186.163704	4013.493812	6.768614	-0.037286	3.456825
186.234480	4021.513787	6.773619	-0.037305	3.460100
186.585809	4029.531449	6.778624	-0.037375	3.463380
186.687654	4037.585787	6.783629	-0.037400	3.466664
187.098266	4045.582048	6.788634	-0.037482	3.469931
187.263782	4053.667533	6.793638	-0.037518	3.473224
187.284846	4061.699041	6.798643	-0.037527	3.476487
187.462976	4069.679647	6.803648	-0.037565	3.479731
187.924532	4077.668032	6.808653	-0.037657	3.482984
188.049427	4085.704948	6.813658	-0.037685	3.486243
188.031955	4093.743514	6.818662	-0.037687	3.489495
188.452912	4101.759509	6.823667	-0.037771	3.492749
188.764429	4109.815606	6.828672	-0.037835	3.496012
188.741986	4117.799822	6.833677	-0.037836	3.499233
189.020153	4125.825638	6.838682	-0.037893	3.502477
189.253736	4133.835304	6.843686	-0.037942	3.505711
189.505639	4141.865052	6.848691	-0.037994	3.508949
189.890064	4149.907005	6.853696	-0.038071	3.512194
190.005489	4157.943589	6.858701	-0.038098	3.515425
190.294166	4165.949583	6.863706	-0.038157	3.518647
190.419329	4173.969966	6.868710	-0.038185	3.521866
190.593887	4181.983108	6.873715	-0.038223	3.525080
190.833695	4190.010453	6.878720	-0.038273	3.528300
190.804490	4198.077933	6.883725	-0.038273	3.531524
191.108761	4206.127042	6.888730	-0.038335	3.534748
191.334446	4214.136289	6.893734	-0.038382	3.537951
191.389684	4222.142091	6.898739	-0.038398	3.541145
191.732824	4230.175335	6.903744	-0.038467	3.544355
191.807481	4238.209225	6.908749	-0.038487	3.547554
192.062573	4246.244938	6.913754	-0.038539	3.550757
192.180564	4254.397987	6.918758	-0.038567	3.553999
192.376609	4262.372588	6.923763	-0.038609	3.557170
192.920963	4270.309189	6.928768	-0.038715	3.560332
192.889099	4278.320436	6.933773	-0.038715	3.563505
193.313581	4286.384472	6.938778	-0.038799	3.566709
193.576414	4294.334229	6.943782	-0.038853	3.569861
193.723086	4302.403116	6.948787	-0.038886	3.573053
194.083590	4310.456717	6.953792	-0.038958	3.576243
194.222114	4318.413305	6.958797	-0.038989	3.579385
194.385677	4326.461552	6.963802	-0.039025	3.582561
194.467763	4334.468918	6.968806	-0.039046	3.585715
194.768280	4342.513023	6.973811	-0.039107	3.588888
195.177686	4350.554244	6.978816	-0.039189	3.592060
195.083471	4358.572551	6.983821	-0.039177	3.595205
195.394101	4366.582673	6.988826	-0.039240	3.598356
195.513781	4374.601514	6.993830	-0.039267	3.601503
195.673532	4382.571167	6.998835	-0.039302	3.604628
195.927919	4390.647330	7.003840	-0.039355	3.607795
196.091350	4398.643612	7.008845	-0.039391	3.610925
196.351611	4406.688124	7.013850	-0.039445	3.614075
196.579506	4414.732430	7.018854	-0.039492	3.617220
196.950086	4422.713847	7.023859	-0.039567	3.620342
197.003402	4430.752388	7.028864	-0.039582	3.623475
197.086741	4438.798250	7.033869	-0.039603	3.626609
197.295105	4446.820008	7.038874	-0.039647	3.629734
197.564518	4454.880758	7.043878	-0.039703	3.632873
197.709095	4462.919353	7.048883	-0.039735	3.635998
197.928407	4470.885744	7.053888	-0.039781	3.639093
198.122384	4478.919585	7.058893	-0.039822	3.642212
198.318769	4486.939270	7.063898	-0.039864	3.645322
198.434570	4494.969746	7.068902	-0.039891	3.648432
198.727089	4503.012162	7.073907	-0.039951	3.651549
198.908015	4511.069915	7.078912	-0.039990	3.654665
198.937740	4519.063042	7.083917	-0.040001	3.657751
199.202907	4527.068231	7.088922	-0.040056	3.660844
199.576815	4535.079541	7.093926	-0.040131	3.663940
199.746972	4543.122729	7.098931	-0.040168	3.667040
200.006111	4551.147409	7.103936	-0.040221	3.670132
200.259045	4559.174515	7.108941	-0.040274	3.673223
200.473053	4567.245241	7.113946	-0.040319	3.676327
200.584028	4575.217306	7.118950	-0.040345	3.679388
200.975617	4583.218403	7.123955	-0.040423	3.682464
201.510927	4591.208817	7.128960	-0.040528	3.685538
201.473852	4599.249186	7.133965	-0.040527	3.688613
201.489305	4607.315717	7.138970	-0.040535	3.691697
201.643330	4615.338325	7.143974	-0.040569	3.694766
201.997681	4623.345732	7.148979	-0.040640	3.697830
202.341572	4631.377822	7.153984	-0.040709	3.700902
202.498920	4639.349213	7.158989	-0.040744	3.703943
202.603142	4647.416776	7.163994	-0.040769	3.707017
202.710492	4655.436698	7.168998	-0.040794	3.710070
202.959400	4663.517550	7.174003	-0.040846	3.713148
203.195719	4671.591219	7.179008	-0.040895	3.716219
203.430134	4679.516230	7.184013	-0.040944	3.719232
203.670706	4687.546246	7.189018	-0.040994	3.722282
203.774018	4695.510790	7.194022	-0.041019	3.725302
204.029963	4703.516019	7.199027	-0.041072	3.728338
204.546235	4711.560359	7.204032	-0.041173	3.731393
204.631290	4719.617714	7.209037	-0.041195	3.734439
204.881796	4727.649918	7.214042	-0.041246	3.737478
204.948826	4735.632243	7.219046	-0.041264	3.740491
205.201512	4743.681674	7.224051	-0.041317	3.743531
205.445152	4751.710961	7.229056	-0.041367	3.746561
205.522744	4759.677368	7.234061	-0.041387	3.749561
205.671259	4767.792043	7.239066	-0.041420	3.752616
205.700550	4775.823408	7.244070	-0.041431	3.755634
206.087296	4783.789646	7.249075	-0.041508	3.758634
206.605196	4791.840249	7.254080	-0.041610	3.761666
206.669289	4799.774958	7.259085	-0.041627	3.764641
206.846374	4807.855959	7.264090	-0.041666	3.767672
207.027771	4815.917423	7.269094	-0.041705	3.770693
207.193120	4823.927092	7.274099	-0.041741	3.773691
207.441944	4832.005956	7.279104	-0.041793	3.776715
207.521102	4839.929134	7.284109	-0.041813	3.779675
207.795023	4847.974315	7.289114	-0.041869	3.782682
208.033779	4855.987876	7.294118	-0.041919	3.785674
207.946220	4864.009442	7.299123	-0.041908	3.788660
208.248885	4872.090839	7.304128	-0.041970	3.791674
208.492857	4880.081437	7.309133	-0.042020	3.794650
208.816322	4888.144414	7.314138	-0.042086	3.797653
208.939143	4896.100196	7.319142	-0.042114	3.800609
209.001964	4904.110320	7.324147	-0.042131	3.803582
209.431660	4912.151977	7.329152	-0.042216	3.806572
209.459979	4920.154023	7.334157	-0.042227	3.809536
209.683818	4928.207690	7.339162	-0.042274	3.812522
209.701039	4936.206908	7.344166	-0.042283	3.815480
209.907762	4944.203283	7.349171	-0.042326	3.818439
210.000009	4952.279262	7.354176	-0.042349	3.821423
210.237995	4960.235711	7.359181	-0.042399	3.824363
210.333011	4968.298773	7.364186	-0.042422	3.827337
210.514388	4976.298882	7.369190	-0.042461	3.830288
210.580740	4984.362576	7.374195	-0.042478	3.833257
210.981119	4992.367286	7.379200	-0.042558	3.836210
210.978480	5000.381969	7.384205	-0.042563	3.839155
211.055025	5008.407798	7.389210	-0.042583	3.842104
211.246769	5016.379874	7.394214	-0.042624	3.845033
211.431352	5024.436880	7.399219	-0.042663	3.847990
211.665125	5032.482143	7.404224	-0.042712	3.850943
211.879981	5040.512536	7.409229	-0.042758	3.853887
212.540867	5048.519871	7.414234	-0.042886	3.856829
212.533427	5056.536385	7.419238	-0.042890	3.859759
212.608818	5064.577627	7.424243	-0.042909	3.862697
212.962294	5072.554496	7.429248	-0.042980	3.865615
213.349462	5080.576006	7.434253	-0.043058	3.868548
213.556875	5088.637344	7.439258	-0.043102	3.871490
213.551644	5096.913470	7.444262	-0.043106	3.874503
213.912134	5104.832500	7.449267	-0.043179	3.877391
214.229167	5112.757307	7.454272	-0.043243	3.880278
214.244994	5120.728024	7.459277	-0.043251	3.883174
214.346650	5128.727753	7.464282	-0.043276	3.886080
214.625249	5136.750143	7.469286	-0.043333	3.888996
214.570103	5144.803738	7.474291	-0.043328	3.891914
214.908711	5152.814569	7.479296	-0.043396	3.894822
215.117273	5160.824424	7.484301	-0.043440	3.897725
215.325029	5168.832616	7.489306	-0.043484	3.900625
215.537547	5176.827609	7.494310	-0.043529	3.903518
215.622480	5184.852419	7.499315	-0.043550	3.906417
215.878522	5192.904860	7.504320	-0.043604	3.909327
215.928686	5200.930500	7.509325	-0.043618	3.912222
216.365369	5208.944416	7.514330	-0.043705	3.915118
216.515612	5216.984876	7.519334	-0.043738	3.918015
216.583438	5224.949528	7.524339	-0.043756	3.920882
216.763405	5232.977892	7.529344	-0.043795	3.923771
217.083215	5240.977517	7.534349	-0.043860	3.926651
217.164738	5249.018396	7.539354	-0.043880	3.929538
217.326748	5257.072600	7.544358	-0.043916	3.932430
217.483040	5265.091266	7.549363	-0.043950	3.935307
217.871778	5273.098450	7.554368	-0.044028	3.938182
217.998101	5281.079011	7.559373	-0.044057	3.941040
218.225363	5289.083255	7.564378	-0.044104	3.943907
218.478547	5297.128885	7.569382	-0.044157	3.946787
218.588022	5305.125300	7.574387	-0.044183	3.949644
218.614537	5313.223413	7.579392	-0.044193	3.952535
218.794023	5321.224739	7.584397	-0.044232	3.955391
219.075235	5329.219231	7.589402	-0.044289	3.958245
219.300527	5337.239796	7.594406	-0.044337	3.961104
219.429780	5345.221616	7.599411	-0.044366	3.963947
219.707328	5353.267294	7.604416	-0.044423	3.966812
219.722331	5361.241478	7.609421	-0.044431	3.969645
219.932549	5369.324918	7.614426	-0.044476	3.972519
220.312929	5377.324591	7.619430	-0.044552	3.975363
220.374541	5385.343049	7.624435	-0.044569	3.978207
220.490870	5393.394747	7.629440	-0.044596	3.981062
220.646544	5401.357860	7.634445	-0.044630	3.983883
220.994388	5409.416848	7.639450	-0.044700	3.986740
221.135696	5417.472550	7.644454	-0.044732	3.989590
221.478042	5425.478182	7.649459	-0.044801	3.992424
221.861694	5433.546197	7.654464	-0.044878	3.995278
221.778739	5441.543563	7.659469	-0.044867	3.998098
222.080979	5449.548058	7.664474	-0.044929	4.000924
222.462514	5457.539772	7.669478	-0.045005	4.003745
222.511667	5465.562559	7.674483	-0.045020	4.006570
222.674688	5473.604696	7.679488	-0.045056	4.009401
222.851603	5481.636884	7.684493	-0.045094	4.012227
223.125794	5489.706163	7.689498	-0.045150	4.015066
223.244853	5497.711456	7.694502	-0.045178	4.017877
223.523772	5505.702185	7.699507	-0.045235	4.020684
223.787619	5513.702832	7.704512	-0.045290	4.023493
223.917463	5521.710439	7.709517	-0.045319	4.026299
224.100458	5529.757133	7.714522	-0.045358	4.029118
224.362016	5537.783016	7.719526	-0.045413	4.031929
224.655495	5545.895483	7.724531	-0.045473	4.034769
224.910602	5553.908102	7.729536	-0.045525	4.037572
224.877413	5561.811342	7.734541	-0.045524	4.040330
225.129582	5569.795006	7.739546	-0.045577	4.043118
225.281639	5577.826057	7.744550	-0.045610	4.045919
225.421840	5585.846196	7.749555	-0.045642	4.048715
225.669008	5593.889111	7.754560	-0.045693	4.051518
225.935935	5601.892906	7.759565	-0.045748	4.054305
226.100440	5609.937922	7.764570	-0.045784	4.057104
226.327219	5617.930315	7.769574	-0.045832	4.059883
226.427525	5625.941451	7.774579	-0.045856	4.062665
226.702155	5633.937673	7.779584	-0.045912	4.065442
226.956620	5641.969119	7.784589	-0.045965	4.068230
227.205528	5649.993784	7.789594	-0.046017	4.071013
227.383135	5658.053018	7.794598	-0.046055	4.073805
227.507808	5666.048603	7.799603	-0.046084	4.076572
227.887216	5674.064173	7.804608	-0.046160	4.079348
228.049605	5682.077488	7.809613	-0.046195	4.082118
228.285666	5690.030155	7.814618	-0.046244	4.084866
228.241732	5698.113985	7.819622	-0.046242	4.087654
228.467702	5706.097914	7.824627	-0.046289	4.090409
228.626534	5714.184159	7.829632	-0.046324	4.093197
228.758738	5722.198974	7.834637	-0.046354	4.095958
228.998170	5730.198896	7.839642	-0.046404	4.098713
229.188389	5738.232490	7.844646	-0.046445	4.101477
229.390222	5746.203889	7.849651	-0.046487	4.104218
229.563005	5754.249098	7.854656	-0.046525	4.106982
229.777818	5762.254569	7.859661	-0.046570	4.109732
229.923645	5770.329048	7.864666	-0.046603	4.112502
230.001881	5778.373211	7.869670	-0.046623	4.115259
230.389372	5786.362382	7.874675	-0.046700	4.117999
230.611975	5794.380309	7.879680	-0.046747	4.120745
230.564597	5802.385018	7.884685	-0.046743	4.123482
230.918422	5810.367064	7.889690	-0.046815	4.126213
231.199679	5818.401021	7.894694	-0.046872	4.128960
231.492605	5826.431805	7.899699	-0.046932	4.131704
231.755573	5834.496580	7.904704	-0.046987	4.134457
231.750102	5842.512024	7.909709	-0.046991	4.137189
231.887830	5850.497561	7.914714	-0.047022	4.139910
232.242116	5858.542460	7.919718	-0.047093	4.142652
232.571239	5866.493612	7.924723	-0.047160	4.145360
232.674640	5874.541390	7.929728	-0.047184	4.148096
232.769119	5882.585640	7.934733	-0.047207	4.150830
233.241579	5890.647395	7.939738	-0.047301	4.153571
233.489599	5898.693628	7.944742	-0.047352	4.156303
233.644210	5906.631357	7.949747	-0.047386	4.158996
233.979202	5914.694656	7.954752	-0.047454	4.161731
234.007511	5922.639692	7.959757	-0.047464	4.164421
234.092556	5930.699735	7.964762	-0.047486	4.167149
234.266570	5938.722499	7.969766	-0.047523	4.169863
234.506607	5946.699454	7.974771	-0.047573	4.172561
234.715970	5954.772380	7.979776	-0.047618	4.175289
234.595421	5962.769541	7.984781	-0.047601	4.177986
234.904165	5970.764743	7.989786	-0.047663	4.180685
235.060527	5978.778374	7.994790	-0.047698	4.183387
235.124396	5986.780671	7.999795	-0.047715	4.186083
235.434888	5994.860317	8.004800	-0.047778	4.188805
235.716933	6002.856160	8.009805	-0.047836	4.191497
235.827706	6011.005606	8.014810	-0.047862	4.194237
236.149628	6018.978282	8.019814	-0.047927	4.196919
236.243416	6026.897963	8.024819	-0.047950	4.199578
236.274258	6034.935387	8.029824	-0.047961	4.202274
236.378380	6042.896623	8.034829	-0.047986	4.204944
236.702188	6050.944084	8.039834	-0.048052	4.207644
237.047659	6058.932786	8.044838	-0.048121	4.210322
236.937259	6066.994193	8.049843	-0.048106	4.213018
237.240267	6074.996413	8.054848	-0.048168	4.215696
237.449982	6083.021501	8.059853	-0.048212	4.218380
237.509002	6091.001871	8.064858	-0.048228	4.221046
237.489514	6099.025111	8.069862	-0.048230	4.223723
237.679674	6107.053135	8.074867	-0.048271	4.226402
237.946165	6115.069204	8.079872	-0.048326	4.229077
238.134959	6123.120758	8.084877	-0.048366	4.231760
238.304621	6131.136758	8.089882	-0.048403	4.234430
238.468609	6139.202173	8.094886	-0.048439	4.237115
238.422853	6147.117869	8.099891	-0.048436	4.239746
238.805746	6155.185712	8.104896	-0.048513	4.242430
238.988515	6163.102435	8.109901	-0.048552	4.245060
239.331107	6171.194937	8.114906	-0.048621	4.247749
239.375737	6179.214911	8.119910	-0.048635	4.250409
239.485428	6187.254243	8.124915	-0.048660	4.253074
239.781896	6195.313597	8.129920	-0.048721	4.255746
239.774240	6203.302049	8.134925	-0.048725	4.258390
239.951373	6211.309602	8.139930	-0.048763	4.261040
240.362167	6219.339877	8.144934	-0.048845	4.263698
240.354711	6227.323538	8.149939	-0.048849	4.266336
240.547974	6235.385610	8.154944	-0.048890	4.268999
240.790469	6243.401414	8.159949	-0.048941	4.271646
241.027022	6251.467903	8.164954	-0.048990	4.274308
241.092186	6259.482130	8.169958	-0.049008	4.276949
241.227651	6267.440842	8.174963	-0.049038	4.279571
241.635127	6275.498512	8.179968	-0.049119	4.282227
241.642149	6283.447515	8.184973	-0.049126	4.284841
241.853394	6291.514339	8.189978	-0.049171	4.287495
242.071804	6299.502430	8.194982	-0.049217	4.290121
242.171399	6307.537287	8.199987	-0.049241	4.292759
242.282249	6315.574971	8.204992	-0.049267	4.295397
242.628457	6323.599866	8.209997	-0.049336	4.298031
242.866418	6331.556057	8.215002	-0.049386	4.300641
242.996272	6339.620701	8.220006	-0.049416	4.303283
243.097478	6347.599404	8.225011	-0.049440	4.305895
243.419322	6355.646851	8.230016	-0.049505	4.308530
243.447379	6363.663783	8.235021	-0.049515	4.311150
243.695299	6371.678913	8.240026	-0.049567	4.313771
244.036357	6379.730493	8.245030	-0.049636	4.316402
244.196216	6387.718268	8.250035	-0.049671	4.319009
244.305317	6395.709145	8.255040	-0.049697	4.321616
244.451187	6403.696461	8.260045	-0.049729	4.324220
244.690457	6411.727945	8.265050	-0.049779	4.326838
244.783517	6419.751100	8.270054	-0.049802	4.329450
244.892556	6427.767299	8.275059	-0.049827	4.332058
245.210891	6435.821616	8.280064	-0.049892	4.334679
245.324241	6443.848521	8.285069	-0.049918	4.337288
245.366972	6451.804771	8.290074	-0.049932	4.339871
245.789998	6459.895941	8.295078	-0.050016	4.342500
246.053676	6467.832553	8.300083	-0.050070	4.345075
246.137574	6475.950875	8.305088	-0.050091	4.347707
246.287069	6483.912871	8.310093	-0.050124	4.350287
246.404100	6491.966129	8.315098	-0.050151	4.352895
246.538175	6500.029745	8.320102	-0.050182	4.355505
246.629439	6508.012124	8.325107	-0.050204	4.358086
247.215714	6515.943862	8.330112	-0.050318	4.360653
247.077457	6523.955479	8.335117	-0.050298	4.363240
247.174780	6531.965662	8.340122	-0.050321	4.365825
247.765243	6540.018407	8.345126	-0.050437	4.368426
247.895480	6547.996077	8.350131	-0.050466	4.370999
248.168506	6556.061342	8.355136	-0.050523	4.373599
248.099534	6564.083046	8.360141	-0.050515	4.376181
248.263990	6572.082240	8.365146	-0.050551	4.378756
248.461852	6580.095370	8.370150	-0.050593	4.381335
248.591174	6588.064884	8.375155	-0.050623	4.383897
248.684834	6596.126226	8.380160	-0.050645	4.386487
249.097029	6604.123053	8.385165	-0.050727	4.389056
249.107035	6612.170062	8.390170	-0.050735	4.391638
249.123300	6620.217824	8.395174	-0.050743	4.394219
249.327005	6628.260607	8.400179	-0.050786	4.396797
249.656593	6636.213645	8.405184	-0.050853	4.399346
249.767790	6644.242050	8.410189	-0.050879	4.401916
249.969716	6652.186966	8.415194	-0.050922	4.404459
250.226917	6660.290080	8.420198	-0.050975	4.407051
250.434408	6668.231668	8.425203	-0.051019	4.409589
250.780786	6676.357832	8.430208	-0.051089	4.412186
250.928421	6684.349850	8.435213	-0.051122	4.414737
250.938475	6692.413092	8.440218	-0.051129	4.417309
251.216679	6700.346093	8.445222	-0.051186	4.419839
251.389512	6708.414573	8.450227	-0.051224	4.422411
251.751862	6716.400951	8.455232	-0.051296	4.424955
251.675254	6724.426302	8.460237	-0.051287	4.427508
251.829649	6732.417926	8.465242	-0.051322	4.430051
252.154107	6740.504400	8.470246	-0.051387	4.432622
252.317378	6748.520066	8.475251	-0.051423	4.435169
252.589975	6756.565622	8.480256	-0.051479	4.437725
252.774654	6764.497908	8.485261	-0.051519	4.440242
252.816645	6772.545795	8.490266	-0.051532	4.442794
252.890781	6780.556571	8.495270	-0.051551	4.445334
253.121974	6788.560290	8.500275	-0.051599	4.447870
253.278041	6796.568544	8.505280	-0.051634	4.450405
253.404087	6804.628164	8.510285	-0.051663	4.452956
253.431770	6812.617493	8.515290	-0.051673	4.455482
253.832571	6820.688389	8.520294	-0.051753	4.458034
253.894072	6828.611440	8.525299	-0.051770	4.460536
254.180261	6836.695922	8.530304	-0.051829	4.463089
254.399832	6844.629430	8.535309	-0.051875	4.465593
254.662841	6852.689868	8.540314	-0.051929	4.468135
254.959686	6860.701163	8.545318	-0.051990	4.470660
255.059206	6868.734873	8.550323	-0.052014	4.473191
255.078558	6876.768971	8.555328	-0.052022	4.475720
255.152223	6884.779333	8.560333	-0.052042	4.478240
255.656239	6892.732758	8.565338	-0.052141	4.480742
255.846354	6900.795969	8.570343	-0.052181	4.483276
255.809047	6908.760375	8.575347	-0.052180	4.485777
255.956099	6916.844080	8.580352	-0.052213	4.488314
256.065222	6924.821237	8.585357	-0.052238	4.490817
256.249387	6932.848114	8.590362	-0.052278	4.493334
256.489697	6940.889100	8.595367	-0.052328	4.495854
256.617982	6948.900653	8.600371	-0.052357	4.498363
256.848439	6956.905002	8.605376	-0.052405	4.500869
257.179011	6964.921175	8.610381	-0.052472	4.503377
257.284333	6972.891596	8.615386	-0.052497	4.505869
257.647084	6980.965667	8.620391	-0.052570	4.508393
257.567640	6988.940346	8.625395	-0.052561	4.510883
258.018214	6997.065081	8.630400	-0.052650	4.513419
258.143341	7005.080472	8.635405	-0.052678	4.515920
258.080476	7013.071449	8.640410	-0.052672	4.518411
258.188850	7021.030736	8.645415	-0.052698	4.520891
258.481083	7029.027500	8.650419	-0.052757	4.523382
258.699792	7037.020166	8.655424	-0.052803	4.525870
258.622385	7045.064062	8.660429	-0.052794	4.528372
258.893498	7053.032265	8.665434	-0.052850	4.530849
259.295856	7061.129938	8.670439	-0.052930	4.533366
259.430111	7069.119897	8.675443	-0.052961	4.535847
259.573097	7077.145444	8.680448	-0.052993	4.538338
259.586117	7085.124678	8.685453	-0.053000	4.540813
259.853823	7093.130405	8.690458	-0.053056	4.543296
260.010334	7101.176332	8.695463	-0.053090	4.545789
260.177033	7109.140993	8.700467	-0.053126	4.548256
260.279758	7117.202091	8.705472	-0.053151	4.550751
260.461279	7125.258316	8.710477	-0.053190	4.553243
260.767707	7133.248952	8.715482	-0.053252	4.555714
260.914027	7141.264733	8.720487	-0.053285	4.558191
260.897702	7149.244933	8.725491	-0.053287	4.560655
261.075530	7157.338231	8.730496	-0.053326	4.563154
261.294056	7165.270943	8.735501	-0.053372	4.565601
261.328506	7173.317784	8.740506	-0.053383	4.568082
261.506456	7181.331248	8.745511	-0.053422	4.570551
261.797471	7189.369208	8.750515	-0.053481	4.573027
261.969462	7197.415888	8.755520	-0.053519	4.575504
261.925568	7205.413494	8.760525	-0.053516	4.577965
262.022658	7213.392889	8.765530	-0.053539	4.580418
262.448258	7221.437268	8.770535	-0.053624	4.582891
262.381859	7229.389947	8.775539	-0.053617	4.585333
262.698137	7237.493122	8.780544	-0.053681	4.587821
262.690926	7245.466591	8.785549	-0.053685	4.590267
262.939266	7253.533894	8.790554	-0.053737	4.592741
263.183052	7261.592407	8.795559	-0.053787	4.595211
263.367844	7269.574808	8.800563	-0.053827	4.597656
263.468857	7277.541101	8.805568	-0.053851	4.600095
263.484370	7285.616734	8.810573	-0.053860	4.602566
263.654042	7293.502837	8.815578	-0.053896	4.604978
264.062591	7301.635524	8.820583	-0.053978	4.607463
264.051546	7309.566797	8.825587	-0.053981	4.609886
264.341017	7317.664265	8.830592	-0.054040	4.612359
264.429363	7325.671732	8.835597	-0.054062	4.614802
264.502745	7333.695745	8.840602	-0.054081	4.617250
264.689381	7341.645400	8.845607	-0.054121	4.619673
264.913234	7349.680362	8.850611	-0.054168	4.622121
265.182031	7357.673640	8.855616	-0.054224	4.624555
265.246390	7365.715858	8.860621	-0.054241	4.627003
265.536694	7373.702429	8.865626	-0.054300	4.629432
266.004685	7381.776019	8.870631	-0.054393	4.631886
265.964089	7389.774358	8.875635	-0.054391	4.634316
266.118693	7397.788859	8.880640	-0.054425	4.636750
266.222594	7405.790998	8.885645	-0.054449	4.639179
266.351631	7413.804679	8.890650	-0.054479	4.641610
266.479642	7421.789661	8.895655	-0.054508	4.644032
266.658157	7429.798655	8.900659	-0.054546	4.646459
267.011138	7437.849790	8.905664	-0.054617	4.648897
267.222667	7445.872676	8.910669	-0.054662	4.651325
267.280920	7453.892926	8.915674	-0.054678	4.653752
267.572423	7461.948493	8.920679	-0.054738	4.656188
267.679741	7469.947529	8.925683	-0.054763	4.658606
267.744258	7477.944341	8.930688	-0.054781	4.661021
267.923354	7485.914943	8.935693	-0.054819	4.663428
268.032189	7493.906927	8.940698	-0.054845	4.665840
268.289764	7501.993014	8.945703	-0.054898	4.668278
268.440539	7509.963662	8.950707	-0.054932	4.670681
268.768852	7518.071225	8.955712	-0.054998	4.673123
268.816461	7526.116008	8.960717	-0.055012	4.675546
268.922656	7534.098986	8.965722	-0.055037	4.677949
269.153966	7542.106705	8.970727	-0.055086	4.680357
269.192336	7550.103774	8.975731	-0.055098	4.682762
269.343769	7558.073591	8.980736	-0.055132	4.685157
269.383582	7566.085180	8.985741	-0.055145	4.687563
269.482787	7574.044159	8.990746	-0.055168	4.689952
269.784784	7582.155582	8.995751	-0.055230	4.692386
269.773221	7590.144896	9.000755	-0.055233	4.694782
270.117029	7598.181871	9.005760	-0.055302	4.697190
270.288736	7606.160156	9.010765	-0.055340	4.699580
270.360533	7614.217836	9.015770	-0.055358	4.701993
270.614867	7622.196798	9.020775	-0.055411	4.704380
270.923040	7630.205463	9.025779	-0.055474	4.706775
270.905801	7638.199649	9.030784	-0.055476	4.709165
271.011129	7646.235633	9.035789	-0.055501	4.711566
271.227161	7654.237107	9.040794	-0.055546	4.713956
271.451305	7662.346372	9.045799	-0.055594	4.716376
271.528017	7670.272119	9.050803	-0.055613	4.718740
271.555324	7678.331217	9.055808	-0.055624	4.721144
271.753687	7686.313462	9.060813	-0.055666	4.723522
271.897489	7694.292945	9.065818	-0.055698	4.725899
272.188288	7702.385075	9.070823	-0.055757	4.728308
272.461120	7710.378425	9.075827	-0.055814	4.730686
272.467548	7718.422256	9.080832	-0.055820	4.733079
272.547319	7726.432145	9.085837	-0.055840	4.735460
272.505106	7734.450991	9.090842	-0.055838	4.737843
272.836206	7742.436226	9.095847	-0.055905	4.740213
272.898494	7750.515984	9.100851	-0.055922	4.742612
273.113334	7758.423860	9.105856	-0.055967	4.744957
273.315002	7766.487209	9.110861	-0.056010	4.747348
273.397051	7774.482612	9.115866	-0.056030	4.749717
273.687226	7782.558499	9.120871	-0.056090	4.752109
273.780640	7790.585394	9.125875	-0.056113	4.754485
273.973859	7798.570187	9.130880	-0.056154	4.756848
274.212805	7806.589202	9.135885	-0.056204	4.759219
274.317257	7814.531274	9.140890	-0.056228	4.761566
274.749236	7822.549461	9.145895	-0.056314	4.763934
274.810440	7830.542308	9.150899	-0.056331	4.766295
275.100273	7838.618554	9.155904	-0.056390	4.768678
275.043455	7846.655874	9.160909	-0.056385	4.771050
275.110806	7854.636518	9.165914	-0.056403	4.773403
275.407392	7862.729401	9.170919	-0.056463	4.775787
275.691550	7870.690595	9.175923	-0.056522	4.778132
275.738874	7878.696762	9.180928	-0.056536	4.780489
275.836525	7886.740571	9.185933	-0.056559	4.782856
276.134850	7894.681138	9.190938	-0.056620	4.785191
276.258606	7902.766328	9.195943	-0.056649	4.787567
276.271508	7910.757130	9.200947	-0.056656	4.789916
276.421877	7918.783853	9.205952	-0.056690	4.792273
276.857078	7926.817125	9.210957	-0.056776	4.794629
276.997976	7934.810281	9.215962	-0.056808	4.796974
277.282003	7942.816195	9.220967	-0.056866	4.799321
277.413757	7950.809718	9.225971	-0.056896	4.801664
277.425553	7958.809410	9.230976	-0.056903	4.804008
277.852666	7966.885263	9.235981	-0.056988	4.806371
277.846269	7974.850985	9.240986	-0.056992	4.808703
278.145099	7982.931653	9.245991	-0.057053	4.811066
278.310656	7990.384015	9.250995	-0.057089	4.813244
278.529369	7994.909654	9.256000	-0.057133	4.814566

278.496089	7997.247299	9.261005	-0.057128	4.815249
278.667241	7998.722526	9.266010	-0.057161	4.815680
278.708562	7999.386745	9.271015	-0.057169	4.815873
278.874564	7999.863074	9.276019	-0.057201	4.816012
278.990128	7999.847018	9.281024	-0.057222	4.816006
278.928903	7999.884381	9.286029	-0.057211	4.816018
278.851843	7999.834914	9.291034	-0.057197	4.816004
279.085326	7999.908610	9.296039	-0.057240	4.816024
279.141185	7999.870102	9.301043	-0.057251	4.816012
279.334175	7999.881095	9.306048	-0.057287	4.816015
279.259544	7999.848766	9.311053	-0.057273	4.816005
279.158447	7999.833052	9.316058	-0.057254	4.816001
279.299097	7999.902927	9.321063	-0.057281	4.816021
279.309530	7999.833678	9.326067	-0.057283	4.816001
279.443477	7999.850009	9.331072	-0.057308	4.816005
279.399822	7999.882349	9.336077	-0.057300	4.816015
279.519851	7999.825774	9.341082	-0.057322	4.815997
279.844177	7999.895779	9.346087	-0.057383	4.816016
279.649528	7999.886914	9.351091	-0.057347	4.816015
279.746268	7999.807478	9.356096	-0.057365	4.815991
279.640332	7999.886768	9.361101	-0.057345	4.816015
279.625310	7999.829878	9.366106	-0.057342	4.815998
279.711317	7999.852818	9.371111	-0.057359	4.816004
279.594652	7999.809042	9.376115	-0.057337	4.815992
279.860839	7999.827774	9.381120	-0.057387	4.815996
279.774289	7999.884978	9.386125	-0.057371	4.816013
279.869083	7999.792686	9.391130	-0.057388	4.815986
279.967347	7999.899189	9.396135	-0.057407	4.816016
279.865550	7999.881324	9.401139	-0.057388	4.816012
280.019698	7999.881996	9.406144	-0.057417	4.816011
280.143395	7999.922718	9.411149	-0.057440	4.816022
280.159910	7999.822593	9.416154	-0.057443	4.815993
280.161178	7999.871775	9.421159	-0.057443	4.816007
280.187468	7999.890427	9.426163	-0.057448	4.816013
280.390642	7999.911222	9.431168	-0.057486	4.816018
280.122754	7999.928806	9.436173	-0.057437	4.816024
280.222780	7999.891100	9.441178	-0.057455	4.816013
280.473636	7999.941610	9.446183	-0.057502	4.816026
280.312440	7999.873516	9.451187	-0.057472	4.816007
280.434550	7999.918483	9.456192	-0.057495	4.816020
280.442356	7999.926115	9.461197	-0.057497	4.816022
280.480273	7999.856294	9.466202	-0.057504	4.816001
280.437992	7999.900413	9.471207	-0.057496	4.816014
280.382136	7999.848123	9.476211	-0.057486	4.815999
280.490463	7999.901387	9.481216	-0.057506	4.816014
280.542040	7999.903402	9.486221	-0.057516	4.816015
280.461765	7999.814340	9.491226	-0.057501	4.815989
280.591570	7999.913939	9.496231	-0.057525	4.816017
280.554587	7999.896182	9.501235	-0.057518	4.816012
280.602437	7999.960102	9.506240	-0.057527	4.816031
280.564789	7999.923100	9.511245	-0.057520	4.816020
280.531219	7999.820996	9.516250	-0.057514	4.815990
280.529202	7999.918201	9.521255	-0.057514	4.816019
280.399333	7999.889141	9.526259	-0.057490	4.816011
280.437475	7999.904803	9.531264	-0.057497	4.816015
280.499658	7999.908080	9.536269	-0.057509	4.816016
280.374138	7999.804306	9.541274	-0.057486	4.815986
280.558432	7999.845060	9.546279	-0.057520	4.815997
280.427635	7999.864064	9.551283	-0.057496	4.816004
280.500091	7999.896376	9.556288	-0.057509	4.816013
280.532448	7999.940782	9.561293	-0.057516	4.816025
280.538652	7999.844742	9.566298	-0.057517	4.815997
280.577453	7999.889265	9.571303	-0.057524	4.816010
280.635762	7999.846527	9.576307	-0.057535	4.815997
280.861559	7999.885898	9.581312	-0.057577	4.816008
280.780079	7999.864127	9.586317	-0.057562	4.816002
280.716354	7999.822378	9.591322	-0.057550	4.815990
280.854582	7999.865501	9.596327	-0.057576	4.816002
280.818393	7999.845622	9.601331	-0.057570	4.815996
280.806259	7999.801605	9.606336	-0.057567	4.815983
280.778300	7999.840641	9.611341	-0.057562	4.815995
280.830079	7999.837318	9.616346	-0.057572	4.815994
281.027673	7999.902889	9.621351	-0.057609	4.816012
280.851489	7999.887946	9.626355	-0.057576	4.816008
280.863689	7999.890315	9.631360	-0.057579	4.816009
280.992191	7999.927920	9.636365	-0.057603	4.816019
280.797504	7999.839984	9.641370	-0.057567	4.815995
280.895824	7999.900547	9.646375	-0.057585	4.816012
280.900849	7999.811965	9.651379	-0.057586	4.815986
281.009520	7999.886606	9.656384	-0.057606	4.816007
281.021990	7999.886843	9.661389	-0.057609	4.816007
280.922839	7999.913901	9.666394	-0.057590	4.816015
280.871021	7999.912970	9.671399	-0.057581	4.816015
280.870366	7999.875572	9.676403	-0.057581	4.816005
281.061018	7999.941018	9.681408	-0.057617	4.816023
280.907524	7999.955336	9.686413	-0.057588	4.816028
280.658202	7999.863202	9.691418	-0.057542	4.816002
280.968434	7999.903039	9.696423	-0.057600	4.816012
281.037189	7999.877586	9.701427	-0.057612	4.816004
281.129614	7999.870727	9.706432	-0.057630	4.816002
281.130265	7999.879298	9.711437	-0.057630	4.816004
280.991770	7999.769944	9.716442	-0.057604	4.815973
281.253505	7999.855913	9.721447	-0.057653	4.815997
281.209520	7999.810249	9.726451	-0.057645	4.815984
281.127184	7999.876078	9.731456	-0.057630	4.816003
281.094026	7999.918226	9.736461	-0.057624	4.816016
281.031195	7999.890383	9.741466	-0.057612	4.816008
281.116857	7999.884470	9.746471	-0.057628	4.816006
281.075066	7999.900817	9.751475	-0.057621	4.816011
281.092430	7999.894732	9.756480	-0.057624	4.816009
281.144270	7999.896753	9.761485	-0.057634	4.816009
281.071188	7999.833463	9.766490	-0.057620	4.815991
281.335254	7999.897038	9.771495	-0.057670	4.816008
281.125852	7999.881491	9.776499	-0.057631	4.816005
281.112960	7999.874856	9.781504	-0.057628	4.816003
281.127143	7999.879398	9.786509	-0.057631	4.816004
281.128984	7999.854867	9.791514	-0.057632	4.815997
281.101818	7999.929178	9.796519	-0.057627	4.816019
281.236558	7999.935910	9.801523	-0.057652	4.816020
281.217382	7999.913134	9.806528	-0.057648	4.816014
281.095245	7999.920542	9.811533	-0.057626	4.816016
280.995211	7999.855695	9.816538	-0.057607	4.815998
281.274766	7999.902454	9.821543	-0.057659	4.816010
281.276918	7999.901435	9.826547	-0.057660	4.816010
281.287396	7999.879198	9.831552	-0.057662	4.816003
281.292606	7999.947687	9.836557	-0.057663	4.816023
281.280446	7999.851312	9.841562	-0.057661	4.815995
281.319804	7999.901188	9.846567	-0.057668	4.816010
281.506628	7999.907798	9.851571	-0.057703	4.816010
281.352183	7999.924236	9.856576	-0.057675	4.816016
281.369330	7999.912804	9.861581	-0.057678	4.816013
281.261138	7999.865972	9.866586	-0.057658	4.816000
281.358065	7999.890182	9.871591	-0.057676	4.816006
281.616233	7999.864965	9.876595	-0.057724	4.815997
281.475496	7999.842117	9.881600	-0.057698	4.815991
281.407924	7999.874023	9.886605	-0.057685	4.816001
281.546571	7999.887238	9.891610	-0.057711	4.816004
281.466559	7999.902890	9.896615	-0.057697	4.816009
281.575050	7999.901666	9.901619	-0.057717	4.816008
281.576116	7999.858956	9.906624	-0.057717	4.815996
281.648187	7999.926523	9.911629	-0.057731	4.816015
281.547139	7999.889437	9.916634	-0.057712	4.816005
281.498622	7999.903525	9.921639	-0.057703	4.816009
281.553927	7999.873554	9.926643	-0.057714	4.816000
281.493824	7999.874610	9.931648	-0.057702	4.816001
281.623257	7999.930397	9.936653	-0.057727	4.816016
281.482555	7999.882974	9.941658	-0.057701	4.816003
281.277300	7999.932680	9.946663	-0.057663	4.816019
281.439865	7999.923891	9.951667	-0.057693	4.816015
281.494889	7999.951613	9.956672	-0.057703	4.816023
281.472902	7999.953361	9.961677	-0.057699	4.816024
281.293395	7999.877453	9.966682	-0.057666	4.816003
281.625965	7999.972191	9.971687	-0.057728	4.816029
281.464451	7999.920116	9.976691	-0.057698	4.816014
281.442224	7999.893010	9.981696	-0.057694	4.816006
281.497552	7999.983780	9.986701	-0.057704	4.816033
281.593341	7999.973777	9.991706	-0.057722	4.816029
281.678383	8000.003114	9.996711	-0.057738	4.816037
281.615892	7999.967797	10.001715	-0.057727	4.816027
281.537500	7999.962109	10.006720	-0.057712	4.816026
281.602700	7999.986811	10.011725	-0.057725	4.816033
281.505794	7999.956211	10.016730	-0.057707	4.816025
281.531987	7999.957766	10.021735	-0.057712	4.816025
281.751979	7999.971391	10.026739	-0.057753	4.816028
281.658254	7999.982520	10.031744	-0.057735	4.816031
281.772359	8000.009180	10.036749	-0.057757	4.816039
281.860975	7999.953101	10.041754	-0.057773	4.816022
281.636072	7999.980011	10.046759	-0.057731	4.816031
281.574019	7999.954319	10.051763	-0.057720	4.816024
281.640469	7999.966222	10.056768	-0.057733	4.816027
281.549139	7999.966710	10.061773	-0.057716	4.816027
281.392049	7999.953181	10.066778	-0.057686	4.816024
281.562881	7999.977665	10.071783	-0.057718	4.816030
281.509245	7999.927550	10.076787	-0.057708	4.816016
281.492228	7999.901607	10.081792	-0.057705	4.816009
281.659808	7999.994417	10.086797	-0.057737	4.816035
281.586827	7999.932197	10.091802	-0.057723	4.816017
281.732069	7999.985066	10.096807	-0.057750	4.816032
281.772351	7999.943068	10.101811	-0.057758	4.816019
281.855619	7999.925358	10.106816	-0.057774	4.816014
281.904801	7999.982894	10.111821	-0.057783	4.816030
281.746715	7999.954387	10.116826	-0.057754	4.816023
281.796096	8000.000173	10.121831	-0.057763	4.816036
281.599650	7999.943188	10.126835	-0.057726	4.816020
281.629551	7999.843302	10.131840	-0.057732	4.815991
281.667495	7999.938031	10.136845	-0.057739	4.816018
281.728544	7999.920986	10.141850	-0.057751	4.816013
281.913058	7999.966021	10.146855	-0.057785	4.816025
281.642117	7999.957903	10.151859	-0.057735	4.816024
281.551170	7999.969083	10.156864	-0.057718	4.816028
281.596512	7999.978465	10.161869	-0.057727	4.816030
281.525597	7999.962228	10.166874	-0.057713	4.816026
281.714636	7999.957125	10.171879	-0.057749	4.816024
281.766318	7999.914266	10.176883	-0.057758	4.816011
281.604983	7999.885701	10.181888	-0.057729	4.816003
281.928987	7999.950367	10.186893	-0.057789	4.816020
281.582835	7999.918443	10.191898	-0.057725	4.816013
281.783064	7999.919955	10.196903	-0.057762	4.816012
281.561230	7999.878537	10.201907	-0.057721	4.816001
281.546705	7999.844092	10.206912	-0.057718	4.815991
281.702703	7999.922800	10.211917	-0.057747	4.816014
281.677759	7999.930905	10.216922	-0.057743	4.816016
281.983339	7999.930057	10.221927	-0.057800	4.816014
281.913413	7999.953373	10.226931	-0.057787	4.816021
281.726828	7999.878403	10.231936	-0.057752	4.816000
281.671302	7999.948994	10.236941	-0.057742	4.816021
281.640989	7999.867248	10.241946	-0.057737	4.815998
281.835873	7999.973376	10.246951	-0.057773	4.816028
281.671773	7999.941555	10.251955	-0.057743	4.816019
281.884707	7999.868502	10.256960	-0.057782	4.815997
281.827699	7999.943341	10.261965	-0.057772	4.816019
281.729483	7999.920196	10.266970	-0.057754	4.816013
281.818451	7999.943194	10.271975	-0.057770	4.816019
281.772636	7999.881467	10.276979	-0.057762	4.816001
281.832701	7999.846239	10.281984	-0.057773	4.815990
281.763703	7999.956121	10.286989	-0.057760	4.816023
281.890232	7999.921033	10.291994	-0.057784	4.816012
282.004689	7999.989371	10.296999	-0.057805	4.816031
281.701941	7999.944345	10.302003	-0.057749	4.816020
281.922068	7999.934465	10.307008	-0.057790	4.816016
281.934432	7999.949659	10.312013	-0.057793	4.816020
281.744775	7999.929127	10.317018	-0.057757	4.816015
281.695080	7999.928234	10.322023	-0.057748	4.816015
281.847159	7999.958790	10.327027	-0.057777	4.816023
281.814937	7999.950735	10.332032	-0.057771	4.816021
281.814704	7999.979591	10.337037	-0.057771	4.816030
281.975080	7999.892761	10.342042	-0.057801	4.816003
282.013058	7999.985354	10.347047	-0.057808	4.816030
282.010909	7999.940448	10.352051	-0.057808	4.816017
282.043052	7999.911124	10.357056	-0.057814	4.816008
281.945888	7999.976685	10.362061	-0.057796	4.816028
281.777462	7999.930894	10.367066	-0.057765	4.816015
282.030383	7999.982516	10.372071	-0.057812	4.816029
281.940966	7999.983038	10.377075	-0.057795	4.816030
281.846411	7999.939658	10.382080	-0.057778	4.816018
281.838432	7999.981196	10.387085	-0.057776	4.816030
281.821886	7999.910384	10.392090	-0.057773	4.816009
281.955227	7999.965174	10.397095	-0.057798	4.816025
281.730407	7999.953620	10.402099	-0.057757	4.816022
281.804162	7999.966724	10.407104	-0.057771	4.816026
281.936327	7999.997986	10.412109	-0.057795	4.816034
282.126533	7999.943754	10.417114	-0.057831	4.816017
282.150672	8000.008314	10.422119	-0.057835	4.816036
282.077695	7999.967463	10.427123	-0.057822	4.816025
282.080935	7999.909832	10.432128	-0.057823	4.816008
282.117648	8000.004540	10.437133	-0.057830	4.816035
281.947470	7999.920250	10.442138	-0.057798	4.816011
282.174715	7999.964994	10.447143	-0.057840	4.816023
282.043742	7999.966898	10.452147	-0.057816	4.816025
282.012923	7999.917197	10.457152	-0.057810	4.816010
282.072872	7999.974928	10.462157	-0.057822	4.816027
281.884271	7999.974717	10.467162	-0.057787	4.816028
281.914318	7999.967794	10.472167	-0.057792	4.816025
282.059676	7999.972583	10.477171	-0.057820	4.816026
282.108412	7999.873038	10.482176	-0.057829	4.815997
282.153164	7999.976440	10.487181	-0.057837	4.816027
282.053234	7999.919071	10.492186	-0.057819	4.816010
282.091167	7999.964649	10.497191	-0.057826	4.816024
281.975590	7999.924092	10.502195	-0.057804	4.816012
281.972521	7999.887718	10.507200	-0.057804	4.816002
282.012703	7999.971802	10.512205	-0.057812	4.816026
282.082603	7999.911109	10.517210	-0.057825	4.816008
281.994432	7999.929819	10.522215	-0.057808	4.816014
282.162749	7999.984178	10.527219	-0.057840	4.816029
282.233637	7999.918160	10.532224	-0.057853	4.816009
282.103084	8000.002348	10.537229	-0.057829	4.816035
281.988559	7999.923343	10.542234	-0.057808	4.816012
282.068537	7999.962205	10.547239	-0.057823	4.816023
282.087368	7999.933708	10.552243	-0.057826	4.816015
282.024388	7999.933642	10.557248	-0.057815	4.816015
282.119059	8000.011239	10.562253	-0.057832	4.816037
282.168787	7999.912780	10.567258	-0.057842	4.816008
282.173614	7999.948140	10.572263	-0.057843	4.816018
282.153450	7999.990525	10.577267	-0.057839	4.816031
282.366934	7999.977319	10.582272	-0.057879	4.816026
282.214001	8000.010880	10.587277	-0.057851	4.816036
282.163430	7999.983258	10.592282	-0.057841	4.816029
282.296086	7999.979268	10.597287	-0.057866	4.816027
282.186116	7999.983691	10.602291	-0.057846	4.816029
281.986826	7999.901009	10.607296	-0.057809	4.816005
282.224403	7999.935256	10.612301	-0.057853	4.816014
282.162470	7999.890331	10.617306	-0.057842	4.816001
282.204755	7999.912481	10.622311	-0.057850	4.816008
282.081462	7999.995732	10.627315	-0.057827	4.816033
282.288150	7999.933251	10.632320	-0.057865	4.816013
282.172525	7999.973901	10.637325	-0.057844	4.816026
282.018125	7999.947598	10.642330	-0.057815	4.816019
282.149898	7999.993812	10.647335	-0.057840	4.816032
281.973594	7999.960700	10.652339	-0.057807	4.816023
281.996763	7999.942967	10.657344	-0.057812	4.816018
282.173904	7999.983595	10.662349	-0.057845	4.816029
282.162561	7999.938521	10.667354	-0.057843	4.816015
282.252875	7999.965818	10.672359	-0.057860	4.816023
282.375195	7999.980874	10.677363	-0.057883	4.816027
282.397028	7999.963116	10.682368	-0.057887	4.816021
282.296496	8000.017931	10.687373	-0.057868	4.816038
282.175594	7999.971935	10.692378	-0.057846	4.816025
282.337298	8000.021899	10.697383	-0.057876	4.816039
282.282555	8000.018778	10.702387	-0.057866	4.816038
282.125700	7999.975333	10.707392	-0.057837	4.816026
282.257862	8000.000185	10.712397	-0.057862	4.816033
282.375623	7999.970280	10.717402	-0.057884	4.816024
282.264567	7999.918051	10.722407	-0.057863	4.816009
282.120493	7999.958184	10.727411	-0.057836	4.816021
282.282792	7999.942980	10.732416	-0.057867	4.816016
282.307256	8000.004341	10.737421	-0.057871	4.816034
282.124672	7999.961497	10.742426	-0.057837	4.816022
282.327176	7999.964120	10.747431	-0.057875	4.816022
282.243391	7999.957265	10.752435	-0.057860	4.816020
282.255254	7999.906202	10.757440	-0.057862	4.816005
282.402532	8000.021084	10.762445	-0.057890	4.816038
282.347750	7999.968810	10.767450	-0.057879	4.816023
282.373288	8000.007751	10.772455	-0.057884	4.816035
282.274466	7999.985664	10.777459	-0.057866	4.816029
282.249841	7999.992706	10.782464	-0.057862	4.816031
282.386580	7999.982380	10.787469	-0.057887	4.816027
282.143325	7999.938434	10.792474	-0.057842	4.816015
282.233841	7999.922993	10.797479	-0.057859	4.816010
282.340024	7999.960194	10.802483	-0.057879	4.816021
282.205096	7999.976986	10.807488	-0.057854	4.816026
282.118508	8000.007478	10.812493	-0.057838	4.816036
282.244375	7999.944597	10.817498	-0.057861	4.816017
282.425813	7999.985303	10.822503	-0.057895	4.816028
282.323683	7999.972772	10.827507	-0.057876	4.816025
282.356675	7999.910339	10.832512	-0.057882	4.816006
282.457488	7999.984842	10.837517	-0.057901	4.816027
282.166307	7999.898352	10.842522	-0.057847	4.816004
282.339808	7999.938914	10.847527	-0.057880	4.816015
282.311481	7999.955506	10.852531	-0.057875	4.816020
282.244305	7999.874157	10.857536	-0.057862	4.815996
282.191159	7999.975779	10.862541	-0.057852	4.816026
282.278345	7999.931428	10.867546	-0.057869	4.816013
282.540499	7999.965054	10.872551	-0.057918	4.816021
282.469479	7999.978733	10.877555	-0.057904	4.816025
282.389186	7999.932405	10.882560	-0.057890	4.816012
282.615761	7999.996372	10.887565	-0.057932	4.816030
282.382187	7999.940847	10.892570	-0.057889	4.816015
282.429790	7999.948134	10.897575	-0.057898	4.816017
282.501846	7999.960140	10.902579	-0.057911	4.816020
282.351731	7999.937120	10.907584	-0.057883	4.816014
282.531264	7999.968175	10.912589	-0.057917	4.816022
282.195299	7999.937503	10.917594	-0.057854	4.816015
282.429710	7999.948185	10.922599	-0.057898	4.816017
282.260476	7999.961148	10.927603	-0.057867	4.816021
282.353952	7999.900883	10.932608	-0.057884	4.816003
282.627045	7999.967832	10.937613	-0.057935	4.816021
282.411760	7999.948969	10.942618	-0.057895	4.816017
282.462544	7999.908230	10.947623	-0.057905	4.816005
282.425292	7999.937483	10.952627	-0.057898	4.816014
282.306314	7999.925714	10.957632	-0.057876	4.816011
282.279425	7999.943401	10.962637	-0.057871	4.816016
282.334392	7999.897395	10.967642	-0.057881	4.816002
282.474896	7999.926672	10.972647	-0.057907	4.816010
282.236611	7999.959750	10.977651	-0.057863	4.816021
282.197892	7999.951577	10.982656	-0.057856	4.816019
282.536379	7999.980179	10.987661	-0.057919	4.816025
282.245902	7999.902250	10.992666	-0.057865	4.816004
282.383090	7999.950701	10.997671	-0.057891	4.816018
282.503516	7999.982819	11.002675	-0.057914	4.816026
282.420360	7999.878739	11.007680	-0.057898	4.815996
282.483120	7999.964304	11.012685	-0.057910	4.816021
282.574347	7999.955288	11.017690	-0.057927	4.816018
282.493901	7999.960247	11.022695	-0.057912	4.816020
282.329861	7999.971167	11.027699	-0.057882	4.816024
282.194951	7999.870421	11.032704	-0.057857	4.815995
282.489574	7999.968748	11.037709	-0.057912	4.816022
282.340608	7999.939338	11.042714	-0.057884	4.816015
282.468791	7999.948089	11.047719	-0.057908	4.816016
282.362459	7999.998525	11.052723	-0.057888	4.816032
282.319429	7999.964629	11.057728	-0.057880	4.816022
282.579853	8000.050582	11.062733	-0.057929	4.816046
282.543024	7999.974057	11.067738	-0.057922	4.816024
282.526172	7999.916060	11.072743	-0.057919	4.816007
282.500035	7999.973296	11.077747	-0.057914	4.816024
282.425363	7999.915317	11.082752	-0.057901	4.816007
282.623716	7999.950989	11.087757	-0.057938	4.816016
282.412118	7999.919372	11.092762	-0.057898	4.816008
282.391190	7999.895494	11.097767	-0.057895	4.816001
282.474795	7999.998535	11.102771	-0.057910	4.816031
282.487530	7999.952830	11.107776	-0.057913	4.816018
282.380808	7999.949832	11.112781	-0.057893	4.816017
282.326723	7999.938174	11.117786	-0.057883	4.816014
282.624118	7999.977783	11.122791	-0.057939	4.816024
282.594104	7999.990070	11.127795	-0.057933	4.816028
282.406434	7999.873406	11.132800	-0.057898	4.815995
282.556837	7999.978729	11.137805	-0.057926	4.816025
282.644689	7999.931183	11.142810	-0.057943	4.816010
282.631298	7999.976898	11.147815	-0.057940	4.816024
282.757027	7999.990948	11.152819	-0.057964	4.816027
282.657442	7999.954955	11.157824	-0.057945	4.816017
282.587429	7999.980406	11.162829	-0.057933	4.816025
282.555188	7999.970213	11.167834	-0.057927	4.816022
282.684891	7999.964033	11.172839	-0.057951	4.816020
282.701855	8000.004957	11.177843	-0.057954	4.816032
282.491975	7999.961616	11.182848	-0.057915	4.816020
282.766302	7999.990121	11.187853	-0.057966	4.816027
282.772761	7999.971015	11.192858	-0.057968	4.816021
282.740801	7999.970445	11.197863	-0.057962	4.816021
282.509159	7999.984409	11.202867	-0.057919	4.816027
282.484855	7999.951922	11.207872	-0.057914	4.816017
282.666394	8000.001180	11.212877	-0.057948	4.816031
282.476243	7999.927210	11.217882	-0.057913	4.816010
282.446615	7999.926682	11.222887	-0.057908	4.816010
282.595857	7999.936885	11.227891	-0.057936	4.816012
282.403786	7999.939816	11.232896	-0.057900	4.816014
282.513494	7999.972808	11.237901	-0.057920	4.816023
282.568869	7999.915055	11.242906	-0.057931	4.816006
282.621929	7999.935264	11.247911	-0.057941	4.816012
282.646119	8000.007306	11.252915	-0.057945	4.816033
282.665261	7999.890126	11.257920	-0.057949	4.815998
282.653341	7999.964717	11.262925	-0.057947	4.816020
282.656065	7999.942338	11.267930	-0.057948	4.816014
282.691386	7999.955813	11.272935	-0.057954	4.816017
282.818507	7999.983779	11.277939	-0.057978	4.816025
282.622971	7999.966344	11.282944	-0.057942	4.816021
282.890532	7999.974424	11.287949	-0.057992	4.816022
282.629935	7999.922681	11.292954	-0.057943	4.816008
282.711735	7999.957304	11.297959	-0.057959	4.816018
282.623261	7999.965323	11.302963	-0.057942	4.816020
282.582903	7999.894076	11.307968	-0.057935	4.816000
282.846082	8000.001450	11.312973	-0.057984	4.816030
282.569774	7999.947285	11.317978	-0.057933	4.816015
282.712950	7999.916774	11.322983	-0.057959	4.816006
282.904818	8000.008961	11.327987	-0.057995	4.816032
282.800341	7999.910903	11.332992	-0.057976	4.816004
282.804731	7999.951598	11.337997	-0.057977	4.816015
282.686849	7999.933438	11.343002	-0.057955	4.816011
282.643505	7999.907015	11.348007	-0.057947	4.816003
282.752703	7999.890846	11.353011	-0.057967	4.815998
282.782010	7999.886046	11.358016	-0.057973	4.815996
283.046337	7999.942152	11.363021	-0.058022	4.816011
282.797809	7999.967563	11.368026	-0.057976	4.816020
282.737474	7999.952586	11.373031	-0.057965	4.816016
282.842036	7999.996170	11.378035	-0.057985	4.816028
282.964352	7999.885139	11.383040	-0.058007	4.815995
283.010027	7999.956504	11.388045	-0.058016	4.816016
282.666514	7999.941721	11.393050	-0.057952	4.816013
282.780679	7999.943807	11.398055	-0.057974	4.816013
282.835456	7999.974732	11.403059	-0.057984	4.816022
282.655529	7999.951170	11.408064	-0.057950	4.816016
282.907604	7999.960037	11.413069	-0.057998	4.816017
282.660914	7999.947014	11.418074	-0.057952	4.816015
282.772436	7999.933024	11.423079	-0.057973	4.816010
282.883297	7999.988477	11.428083	-0.057993	4.816026
282.747695	7999.913362	11.433088	-0.057968	4.816005
282.753114	8000.004297	11.438093	-0.057969	4.816031
282.741954	7999.974185	11.443098	-0.057967	4.816022
282.915035	7999.962382	11.448103	-0.058000	4.816018
282.859681	7999.983826	11.453107	-0.057989	4.816025
282.763067	7999.937201	11.458112	-0.057972	4.816011
283.044363	7999.980793	11.463117	-0.058024	4.816023
282.630837	7999.924133	11.468122	-0.057947	4.816008
282.764256	7999.956488	11.473127	-0.057972	4.816017
282.796209	7999.989136	11.478131	-0.057978	4.816026
282.718827	7999.896914	11.483136	-0.057964	4.816000
282.874697	7999.869839	11.488141	-0.057993	4.815991
282.853073	7999.932500	11.493146	-0.057989	4.816010
282.840730	7999.948314	11.498151	-0.057987	4.816014
282.797726	7999.959297	11.503155	-0.057979	4.816018
282.811004	7999.900779	11.508160	-0.057982	4.816000
282.948955	7999.918257	11.513165	-0.058007	4.816005
282.875155	7999.925474	11.518170	-0.057994	4.816007
282.719760	7999.906631	11.523175	-0.057965	4.816003
282.859343	7999.944441	11.528179	-0.057991	4.816013
282.939026	7999.970477	11.533184	-0.058006	4.816020
283.000883	7999.954515	11.538189	-0.058018	4.816015
282.908966	7999.958197	11.543194	-0.058001	4.816017
283.040911	7999.970223	11.548199	-0.058025	4.816020
282.941472	7999.997277	11.553203	-0.058007	4.816028
282.844952	7999.938900	11.558208	-0.057989	4.816011
283.044615	7999.997036	11.563213	-0.058026	4.816027
282.905653	7999.938956	11.568218	-0.058000	4.816011
282.932414	7999.927699	11.573223	-0.058006	4.816008
283.007100	7999.951506	11.578227	-0.058020	4.816014
282.909053	7999.857840	11.583232	-0.058001	4.815987
282.996090	7999.968424	11.588237	-0.058018	4.816019
283.094428	7999.971291	11.593242	-0.058036	4.816020
283.049590	7999.914922	11.598247	-0.058028	4.816003
283.080229	7999.963574	11.603251	-0.058034	4.816017
283.071130	7999.860839	11.608256	-0.058032	4.815987
283.101144	7999.930850	11.613261	-0.058038	4.816008
282.858772	7999.926454	11.618266	-0.057993	4.816008
282.726715	7999.849267	11.623271	-0.057968	4.815986
282.875792	7999.928922	11.628275	-0.057996	4.816008
282.880312	7999.812544	11.633280	-0.057997	4.815974
282.950864	7999.865126	11.638285	-0.058010	4.815989
283.076589	7999.895205	11.643290	-0.058034	4.815997
282.912773	7999.812097	11.648295	-0.058003	4.815974
282.886348	7999.899247	11.653299	-0.057999	4.816000
282.977751	7999.899850	11.658304	-0.058016	4.815999
283.188065	7999.946426	11.663309	-0.058055	4.816012
283.078058	7999.901695	11.668314	-0.058035	4.815999
283.090714	7999.870948	11.673319	-0.058037	4.815990
283.063915	7999.930309	11.678323	-0.058032	4.816008
283.037400	7999.908467	11.683328	-0.058027	4.816001
283.123261	7999.935684	11.688333	-0.058044	4.816009
283.076990	7999.899591	11.693338	-0.058035	4.815999
283.072049	7999.866387	11.698343	-0.058034	4.815989
283.085993	7999.931832	11.703347	-0.058037	4.816008
283.024528	7999.887983	11.708352	-0.058026	4.815995
283.096939	7999.910681	11.713357	-0.058039	4.816002
282.995000	7999.851137	11.718362	-0.058020	4.815985
283.041581	7999.865885	11.723367	-0.058029	4.815989
282.982017	7999.937474	11.728371	-0.058018	4.816010
283.061490	7999.836349	11.733376	-0.058033	4.815980
283.116929	7999.924988	11.738381	-0.058043	4.816006
283.074767	7999.882559	11.743386	-0.058036	4.815994
283.145958	7999.872109	11.748391	-0.058049	4.815990
283.102715	7999.921555	11.753395	-0.058041	4.816005
283.080182	7999.899785	11.758400	-0.058037	4.815999
283.173348	7999.943163	11.763405	-0.058055	4.816011
282.976334	7999.936386	11.768410	-0.058018	4.816010
283.034221	7999.879747	11.773415	-0.058029	4.815993
283.122305	7999.982871	11.778419	-0.058045	4.816023
283.031769	7999.898957	11.783424	-0.058029	4.815999
282.975247	7999.962053	11.788429	-0.058018	4.816017
282.911222	7999.930980	11.793434	-0.058006	4.816009
282.961916	7999.885965	11.798439	-0.058016	4.815995
282.935772	7999.945339	11.803443	-0.058011	4.816013
282.920895	7999.891652	11.808448	-0.058008	4.815997
283.076200	7999.973558	11.813453	-0.058038	4.816020
283.137317	7999.952240	11.818458	-0.058049	4.816014
283.163985	7999.907856	11.823463	-0.058054	4.816000
282.925254	7999.918486	11.828467	-0.058010	4.816005
282.996475	7999.877050	11.833472	-0.058023	4.815992
283.178366	7999.893190	11.838477	-0.058057	4.815996
283.042846	7999.921724	11.843482	-0.058032	4.816005
282.948186	7999.930699	11.848487	-0.058014	4.816008
283.255776	7999.976907	11.853491	-0.058072	4.816020
283.154499	7999.900277	11.858496	-0.058053	4.815998
283.073937	7999.945839	11.863501	-0.058038	4.816012
283.148369	7999.900187	11.868506	-0.058052	4.815998
283.100698	7999.859795	11.873511	-0.058043	4.815987
283.114237	7999.891039	11.878515	-0.058046	4.815996
283.108029	7999.920856	11.883520	-0.058045	4.816005
282.991180	7999.906988	11.888525	-0.058023	4.816001
282.798170	7999.931272	11.893530	-0.057987	4.816009
283.251162	7999.864720	11.898535	-0.058072	4.815987
283.216025	7999.955986	11.903539	-0.058065	4.816014
283.052849	7999.929522	11.908544	-0.058035	4.816007
283.243385	7999.968259	11.913549	-0.058071	4.816018
283.229209	7999.954121	11.918554	-0.058068	4.816014
283.055161	7999.927458	11.923559	-0.058036	4.816007
282.896312	7999.937403	11.928563	-0.058006	4.816010
282.910286	7999.904543	11.933568	-0.058009	4.816001
283.154057	7999.973098	11.938573	-0.058055	4.816020
282.841474	7999.953535	11.943578	-0.057997	4.816015
283.141313	7999.901295	11.948583	-0.058053	4.815999
283.273830	7999.839602	11.953587	-0.058077	4.815980
283.144677	7999.808414	11.958592	-0.058053	4.815971
283.176487	7999.904103	11.963597	-0.058059	4.815999
283.071251	7999.925708	11.968602	-0.058040	4.816006
282.952071	7999.926758	11.973607	-0.058018	4.816007
283.091508	7999.983799	11.978611	-0.058044	4.816023
283.028336	7999.911068	11.983616	-0.058032	4.816002
283.153840	7999.929389	11.988621	-0.058056	4.816007
283.076006	7999.936533	11.993626	-0.058041	4.816009
283.071395	7999.988818	11.998631	-0.058041	4.816025
283.123616	7999.941693	12.003635	-0.058050	4.816010
282.962588	7999.870389	12.008640	-0.058020	4.815990
283.189111	7999.956796	12.013645	-0.058063	4.816015
283.391992	7999.978661	12.018650	-0.058101	4.816020
283.253830	7999.856482	12.023655	-0.058075	4.815985
283.387965	7999.968992	12.028659	-0.058100	4.816017
283.163141	7999.891185	12.033664	-0.058058	4.815995
283.325945	7999.956131	12.038669	-0.058089	4.816014
283.278121	7999.952066	12.043674	-0.058080	4.816013
283.162732	7999.858084	12.048679	-0.058059	4.815986
283.254865	7999.942047	12.053683	-0.058076	4.816010
283.200406	7999.947479	12.058688	-0.058066	4.816012
283.188385	7999.991082	12.063693	-0.058064	4.816025
283.248173	7999.937683	12.068698	-0.058075	4.816009
283.203807	7999.918721	12.073703	-0.058067	4.816003
283.317575	7999.966748	12.078707	-0.058088	4.816017
283.359983	7999.901280	12.083712	-0.058096	4.815997
283.253539	7999.938891	12.088717	-0.058076	4.816009
283.183062	7999.999596	12.093722	-0.058063	4.816027
283.356177	7999.985658	12.098727	-0.058096	4.816022
283.282373	7999.993943	12.103731	-0.058082	4.816025
283.086766	7999.929489	12.108736	-0.058046	4.816007
283.181029	8000.018835	12.113741	-0.058064	4.816033
283.173031	7999.990918	12.118746	-0.058062	4.816025
283.135315	7999.935746	12.123751	-0.058055	4.816009
283.120109	7999.991045	12.128755	-0.058052	4.816025
283.025542	7999.898510	12.133760	-0.058035	4.815998
283.299181	8000.003939	12.138765	-0.058086	4.816028
283.202815	7999.969072	12.143770	-0.058068	4.816018
283.218562	7999.908462	12.148775	-0.058071	4.816000
283.324606	7999.977719	12.153779	-0.058091	4.816020
283.219314	7999.962992	12.158784	-0.058072	4.816016
283.124890	8000.024330	12.163789	-0.058054	4.816035
283.228183	8000.003780	12.168794	-0.058073	4.816028
283.408015	7999.986758	12.173799	-0.058107	4.816022
283.433893	7999.950908	12.178803	-0.058112	4.816011
283.368016	7999.910184	12.183808	-0.058100	4.816000
283.359232	7999.972011	12.188813	-0.058098	4.816018
283.218661	7999.961985	12.193818	-0.058072	4.816016
283.226399	7999.929011	12.198823	-0.058074	4.816006
283.357240	8000.001926	12.203827	-0.058098	4.816027
283.310101	7999.884607	12.208832	-0.058090	4.815993
283.238340	7999.922849	12.213837	-0.058076	4.816004
283.135859	7999.958395	12.218842	-0.058057	4.816015
283.262444	7999.884840	12.223847	-0.058081	4.815993
283.192604	7999.943419	12.228851	-0.058068	4.816010
283.096301	7999.965187	12.233856	-0.058050	4.816017
283.428242	7999.932765	12.238861	-0.058112	4.816006
283.282035	7999.923706	12.243866	-0.058085	4.816004
283.193172	7999.945609	12.248871	-0.058069	4.816011
283.297771	8000.008429	12.253875	-0.058088	4.816029
283.385739	7999.905321	12.258880	-0.058105	4.815998
283.302691	7999.957249	12.263885	-0.058089	4.816014
283.368725	7999.945637	12.268890	-0.058102	4.816010
283.280948	7999.911995	12.273895	-0.058085	4.816001
283.343827	7999.985811	12.278899	-0.058097	4.816022
283.124572	7999.933749	12.283904	-0.058057	4.816008
283.302959	7999.970129	12.288909	-0.058090	4.816018
283.128325	7999.939181	12.293914	-0.058058	4.816010
283.187592	7999.884705	12.298919	-0.058069	4.815993
283.278169	7999.986806	12.303923	-0.058086	4.816023
283.483734	7999.960635	12.308928	-0.058124	4.816014
283.422752	7999.980908	12.313933	-0.058113	4.816020
283.299414	7999.972264	12.318938	-0.058090	4.816018
283.448420	7999.885226	12.323943	-0.058118	4.815992
283.638338	8000.003026	12.328947	-0.058153	4.816025
283.329494	7999.948266	12.333952	-0.058096	4.816011
283.716991	7999.956392	12.338957	-0.058168	4.816011
283.493488	7999.995080	12.343962	-0.058127	4.816024
283.318793	7999.951308	12.348967	-0.058094	4.816012
283.462609	7999.984922	12.353971	-0.058121	4.816021
283.469869	7999.931637	12.358976	-0.058123	4.816005
283.501597	7999.968555	12.363981	-0.058129	4.816016
283.390713	7999.927013	12.368986	-0.058108	4.816005
283.517744	7999.958184	12.373991	-0.058132	4.816013
283.510009	7999.952711	12.378995	-0.058130	4.816011
283.387644	7999.965456	12.384000	-0.058108	4.816016
283.580335	7999.972177	12.389005	-0.058144	4.816017
283.507905	7999.992241	12.394010	-0.058130	4.816023
283.220156	7999.883370	12.399015	-0.058077	4.815993
283.409648	7999.988338	12.404019	-0.058112	4.816022
283.358650	7999.955365	12.409024	-0.058103	4.816013
283.318550	7999.892670	12.414029	-0.058095	4.815995
283.277039	7999.896200	12.419034	-0.058088	4.815996
283.305174	7999.844363	12.424039	-0.058093	4.815981
283.419638	7999.933007	12.429043	-0.058115	4.816006
283.288961	7999.932779	12.434048	-0.058090	4.816007
283.472282	7999.982071	12.439053	-0.058125	4.816020
283.514436	7999.981779	12.444058	-0.058133	4.816020
283.542537	7999.969478	12.449063	-0.058138	4.816016
283.458834	7999.991475	12.454067	-0.058123	4.816023
283.379436	7999.914174	12.459072	-0.058108	4.816001
283.446495	7999.938912	12.464077	-0.058120	4.816008
283.268485	7999.936754	12.469082	-0.058087	4.816008
283.408715	7999.991674	12.474087	-0.058114	4.816023
283.404464	8000.038624	12.479091	-0.058113	4.816037
283.302536	7999.990832	12.484096	-0.058094	4.816024
283.300189	7999.980115	12.489101	-0.058094	4.816020
283.311977	7999.905541	12.494106	-0.058096	4.815999
283.520397	7999.901861	12.499111	-0.058135	4.815996
283.581173	7999.955336	12.504115	-0.058146	4.816012
283.557746	7999.942098	12.509120	-0.058142	4.816008
283.591588	7999.943792	12.514125	-0.058149	4.816008
283.385850	7999.996695	12.519130	-0.058110	4.816025
283.301347	7999.985552	12.524135	-0.058095	4.816022
283.696198	7999.966029	12.529139	-0.058168	4.816014
283.369566	7999.895986	12.534144	-0.058108	4.815995
283.546689	7999.904560	12.539149	-0.058141	4.815997
283.577515	7999.907268	12.544154	-0.058147	4.815998
283.541340	7999.898073	12.549159	-0.058140	4.815995
283.533957	8000.009079	12.554163	-0.058139	4.816028
283.454068	7999.996951	12.559168	-0.058124	4.816025
283.628537	7999.925335	12.564173	-0.058156	4.816003
283.470040	7999.962000	12.569178	-0.058127	4.816014
283.469773	7999.910715	12.574183	-0.058127	4.815999
283.619948	7999.991461	12.579187	-0.058155	4.816022
283.605801	7999.968775	12.584192	-0.058153	4.816015
283.532214	7999.967447	12.589197	-0.058139	4.816015
283.563583	7999.979782	12.594202	-0.058145	4.816019
283.652767	7999.918369	12.599207	-0.058162	4.816000
283.562197	7999.933830	12.604211	-0.058145	4.816005
283.420787	7999.953708	12.609216	-0.058119	4.816012
283.506577	7999.918948	12.614221	-0.058135	4.816001
283.496742	7999.944425	12.619226	-0.058133	4.816009
283.454120	7999.951140	12.624231	-0.058125	4.816011
283.536025	7999.970806	12.629235	-0.058141	4.816016
283.310183	7999.936790	12.634240	-0.058099	4.816008
283.503447	7999.989468	12.639245	-0.058135	4.816022
283.581670	7999.983422	12.644250	-0.058149	4.816020
283.424190	7999.953854	12.649255	-0.058120	4.816012
283.402975	7999.989810	12.654259	-0.058116	4.816023
283.395606	7999.969384	12.659264	-0.058115	4.816017
283.578510	7999.972720	12.664269	-0.058149	4.816017
283.502618	7999.941431	12.669274	-0.058135	4.816008
283.437721	7999.904999	12.674279	-0.058123	4.815998
283.743032	7999.921247	12.679283	-0.058180	4.816001
283.681709	7999.948994	12.684288	-0.058169	4.816009
283.699511	7999.937574	12.689293	-0.058172	4.816006
283.609013	7999.970132	12.694298	-0.058156	4.816016
283.570312	7999.881817	12.699303	-0.058148	4.815990
283.537753	7999.984886	12.704307	-0.058143	4.816020
283.648464	7999.940961	12.709312	-0.058163	4.816007
283.581999	7999.948312	12.714317	-0.058151	4.816010
283.509505	7999.956621	12.719322	-0.058138	4.816012
283.409852	7999.917420	12.724327	-0.058119	4.816001
283.616237	7999.986366	12.729331	-0.058158	4.816020
283.501712	7999.944757	12.734336	-0.058136	4.816009
283.535569	7999.957137	12.739341	-0.058143	4.816012
283.458296	7999.938645	12.744346	-0.058129	4.816007
283.673408	7999.879522	12.749351	-0.058169	4.815989
283.555923	8000.002418	12.754355	-0.058147	4.816025
283.385229	7999.953376	12.759360	-0.058115	4.816012
283.497658	7999.994968	12.764365	-0.058136	4.816024
283.459511	7999.972914	12.769370	-0.058129	4.816017
283.376602	7999.932948	12.774375	-0.058114	4.816006
283.470468	8000.015876	12.779379	-0.058132	4.816030
283.533134	7999.993518	12.784384	-0.058143	4.816023
283.548956	7999.911537	12.789389	-0.058146	4.815999
283.547557	7999.944647	12.794394	-0.058146	4.816009
283.539237	7999.956261	12.799399	-0.058145	4.816012
283.732096	7999.952299	12.804403	-0.058181	4.816010
283.635169	7999.958026	12.809408	-0.058163	4.816012
283.773232	7999.891091	12.814413	-0.058189	4.815992
283.670148	7999.986466	12.819418	-0.058170	4.816020
283.468965	7999.943281	12.824423	-0.058132	4.816009
283.679780	7999.988800	12.829427	-0.058172	4.816021
283.676438	7999.888304	12.834432	-0.058171	4.815991
283.667044	7999.974698	12.839437	-0.058170	4.816017
283.611866	7999.908522	12.844442	-0.058159	4.815998
283.643961	7999.915528	12.849447	-0.058165	4.816000
283.610593	8000.017514	12.854451	-0.058159	4.816030
283.697457	7999.967813	12.859456	-0.058176	4.816015
283.634016	7999.949572	12.864461	-0.058164	4.816010
283.667552	8000.001484	12.869466	-0.058170	4.816025
283.546290	7999.945861	12.874471	-0.058148	4.816009
283.723904	7999.986501	12.879475	-0.058181	4.816020
283.672981	7999.917197	12.884480	-0.058172	4.816000
283.536930	7999.932899	12.889485	-0.058146	4.816005
283.673818	7999.969593	12.894490	-0.058172	4.816015
283.618981	7999.933344	12.899495	-0.058162	4.816005
283.648837	7999.943514	12.904499	-0.058168	4.816008
283.521626	7999.941211	12.909504	-0.058144	4.816008
283.567870	7999.992285	12.914509	-0.058153	4.816022
283.952093	8000.007833	12.919514	-0.058224	4.816025
283.614889	7999.941870	12.924519	-0.058162	4.816007
283.870744	8000.015991	12.929523	-0.058209	4.816028
283.834491	7999.939474	12.934528	-0.058203	4.816005
283.765889	7999.898700	12.939533	-0.058190	4.815994
283.672745	7999.998530	12.944538	-0.058173	4.816024
283.597935	8000.010003	12.949543	-0.058159	4.816027
283.677894	8000.031770	12.954547	-0.058174	4.816033
283.536776	7999.990746	12.959552	-0.058148	4.816022
283.618838	7999.920655	12.964557	-0.058163	4.816001
283.761719	8000.004475	12.969562	-0.058190	4.816025
283.518744	7999.895347	12.974567	-0.058145	4.815994
283.690998	8000.014964	12.979571	-0.058177	4.816028
283.768484	7999.980052	12.984576	-0.058192	4.816018
283.821191	7999.973541	12.989581	-0.058201	4.816015
283.824046	8000.003524	12.994586	-0.058202	4.816024
283.706393	7999.942623	12.999591	-0.058180	4.816007
283.715670	8000.001574	13.004595	-0.058182	4.816024
283.598455	7999.980218	13.009600	-0.058160	4.816019
283.761649	8000.001362	13.014605	-0.058191	4.816024
283.897957	8000.016675	13.019610	-0.058216	4.816028
283.624160	7999.911260	13.024615	-0.058166	4.815998
283.783668	8000.005000	13.029619	-0.058195	4.816025
283.785655	8000.006115	13.034624	-0.058196	4.816025
283.850323	8000.003028	13.039629	-0.058208	4.816024
283.693895	8000.002330	13.044634	-0.058179	4.816025
283.792910	7999.983839	13.049639	-0.058198	4.816019
283.751725	8000.021569	13.054643	-0.058190	4.816030
283.607224	7999.981551	13.059648	-0.058163	4.816019
283.566548	7999.978685	13.064653	-0.058156	4.816018
283.779874	7999.943038	13.069658	-0.058195	4.816007
283.745111	7999.867617	13.074663	-0.058189	4.815985
283.761371	7999.944859	13.079667	-0.058192	4.816007
283.770136	7999.925795	13.084672	-0.058194	4.816002
283.920403	7999.927470	13.089677	-0.058222	4.816001
283.834867	7999.949433	13.094682	-0.058206	4.816008
283.720477	7999.921718	13.099687	-0.058185	4.816001
283.929466	7999.920186	13.104691	-0.058224	4.815999
283.762488	7999.909680	13.109696	-0.058193	4.815997
283.820147	7999.933179	13.114701	-0.058204	4.816004
283.940857	8000.003774	13.119706	-0.058227	4.816024
283.882996	7999.873435	13.124711	-0.058216	4.815986
283.932739	7999.920298	13.129715	-0.058225	4.815999
283.915019	7999.975552	13.134720	-0.058222	4.816015
283.999177	8000.002739	13.139725	-0.058238	4.816023
283.864444	8000.001368	13.144730	-0.058213	4.816023
283.701096	7999.971693	13.149735	-0.058183	4.816015
283.717491	8000.017950	13.154739	-0.058186	4.816029
283.604808	7999.996677	13.159744	-0.058165	4.816023
283.708056	7999.929108	13.164749	-0.058184	4.816003
283.670011	7999.990404	13.169754	-0.058177	4.816021
283.587277	7999.952578	13.174759	-0.058162	4.816010
283.686881	8000.020651	13.179763	-0.058181	4.816030
283.624210	7999.999219	13.184768	-0.058169	4.816024
283.716063	8000.013723	13.189773	-0.058186	4.816028
283.633004	8000.016497	13.194778	-0.058171	4.816029
283.448950	7999.982172	13.199783	-0.058137	4.816020
283.558583	8000.029056	13.204787	-0.058157	4.816033
283.572904	7999.964144	13.209792	-0.058160	4.816014
283.558889	7999.956420	13.214797	-0.058157	4.816012
283.534941	7999.979503	13.219802	-0.058153	4.816019
283.570954	7999.907507	13.224807	-0.058160	4.815997
283.738526	7999.980021	13.229811	-0.058191	4.816018
283.611936	7999.987347	13.234816	-0.058168	4.816020
283.756916	7999.980377	13.239821	-0.058195	4.816018
283.689807	7999.977030	13.244826	-0.058182	4.816017
283.708107	7999.950659	13.249831	-0.058186	4.816009
283.768568	8000.004129	13.254835	-0.058197	4.816025
283.535066	8000.003098	13.259840	-0.058154	4.816025
283.550364	7999.965987	13.264845	-0.058157	4.816015
283.714120	7999.954016	13.269850	-0.058188	4.816010
283.627019	7999.928934	13.274855	-0.058171	4.816003
283.692335	7999.972875	13.279859	-0.058184	4.816016
283.552803	7999.987445	13.284864	-0.058158	4.816021
283.705050	7999.902602	13.289869	-0.058186	4.815995
283.653185	7999.997840	13.294874	-0.058177	4.816023
283.537664	7999.948732	13.299879	-0.058155	4.816010
283.671293	7999.973613	13.304883	-0.058180	4.816016
283.737821	7999.978039	13.309888	-0.058193	4.816017
283.591662	7999.902729	13.314893	-0.058166	4.815996
283.891924	7999.969109	13.319898	-0.058222	4.816014
283.769522	7999.895299	13.324903	-0.058199	4.815993
283.899266	7999.989566	13.329907	-0.058223	4.816020
283.701781	7999.945379	13.334912	-0.058187	4.816008
283.763436	7999.919797	13.339917	-0.058198	4.816000
283.800489	7999.962155	13.344922	-0.058205	4.816012
283.961613	7999.878542	13.349927	-0.058235	4.815987
284.014979	7999.968215	13.354931	-0.058245	4.816013
283.888434	7999.985158	13.359936	-0.058222	4.816018
283.794380	7999.963155	13.364941	-0.058205	4.816012
284.090979	8000.005960	13.369946	-0.058260	4.816023
283.999481	7999.897449	13.374951	-0.058243	4.815992
284.085465	7999.911846	13.379955	-0.058259	4.815996
283.800363	7999.877820	13.384960	-0.058206	4.815987
283.873811	7999.956103	13.389965	-0.058220	4.816010
283.899263	8000.012143	13.394970	-0.058225	4.816026
283.804763	7999.967691	13.399975	-0.058207	4.816014
283.885501	8000.014050	13.404979	-0.058222	4.816027
284.009853	7999.972511	13.409984	-0.058246	4.816014
283.874853	7999.957243	13.414989	-0.058221	4.816010
283.760669	7999.982960	13.419994	-0.058199	4.816018
283.842713	7999.940651	13.424999	-0.058215	4.816005
283.910705	8000.028453	13.430003	-0.058228	4.816031
283.626803	8000.002996	13.435008	-0.058175	4.816025
283.913346	7999.954790	13.440013	-0.058228	4.816009
283.910995	7999.990021	13.445018	-0.058228	4.816020
283.776715	8000.001480	13.450023	-0.058203	4.816024
284.010396	8000.063445	13.455027	-0.058247	4.816040
283.984716	7999.990325	13.460032	-0.058242	4.816019
283.825039	7999.922248	13.465037	-0.058212	4.816000
283.733444	8000.013558	13.470042	-0.058195	4.816027
283.874075	7999.939189	13.475047	-0.058222	4.816005
283.944547	7999.924453	13.480051	-0.058235	4.816000
283.755347	7999.953079	13.485056	-0.058200	4.816010
283.893609	7999.964153	13.490061	-0.058226	4.816012
283.826628	7999.999277	13.495066	-0.058213	4.816023
283.658632	7999.912883	13.500071	-0.058182	4.815998
283.749250	7999.973313	13.505075	-0.058199	4.816015
283.952483	7999.977020	13.510080	-0.058237	4.816015
283.853448	7999.926075	13.515085	-0.058219	4.816001
283.923573	8000.003230	13.520090	-0.058232	4.816023
283.899842	7999.949380	13.525095	-0.058228	4.816008
283.874364	7999.968161	13.530099	-0.058223	4.816013
283.847987	7999.996544	13.535104	-0.058218	4.816022
284.004223	7999.939556	13.540109	-0.058247	4.816004
284.057204	7999.959764	13.545114	-0.058257	4.816010
283.979834	7999.931653	13.550119	-0.058243	4.816002
283.920798	7999.987224	13.555123	-0.058232	4.816019
283.923088	7999.976591	13.560128	-0.058233	4.816015
283.831519	7999.955701	13.565133	-0.058216	4.816010
283.961042	8000.015771	13.570138	-0.058240	4.816027
283.841660	7999.984758	13.575143	-0.058218	4.816018
284.212930	8000.003277	13.580147	-0.058287	4.816022
284.071494	7999.963314	13.585152	-0.058261	4.816011
284.062212	7999.890492	13.590157	-0.058259	4.815990
284.216492	8000.003373	13.595162	-0.058288	4.816022
284.024698	7999.934711	13.600167	-0.058252	4.816003
283.937759	7999.975883	13.605171	-0.058236	4.816015
283.972697	7999.971186	13.610176	-0.058243	4.816014
283.894799	7999.951614	13.615181	-0.058229	4.816008
283.769837	7999.972860	13.620186	-0.058205	4.816015
283.740287	7999.919973	13.625191	-0.058200	4.816000
283.902055	8000.011618	13.630195	-0.058230	4.816026
283.851809	7999.920954	13.635200	-0.058221	4.816000
283.970323	7999.915640	13.640205	-0.058243	4.815997
284.087036	7999.997917	13.645210	-0.058265	4.816021
284.008809	7999.915293	13.650215	-0.058251	4.815997
283.816296	7999.924625	13.655219	-0.058215	4.816001
283.762043	7999.953568	13.660224	-0.058205	4.816010
283.798396	7999.948897	13.665229	-0.058212	4.816008
283.643764	7999.996318	13.670234	-0.058183	4.816023
283.834468	7999.927134	13.675239	-0.058219	4.816001
283.878250	7999.970684	13.680243	-0.058227	4.816014
283.889582	7999.951666	13.685248	-0.058229	4.816008
283.743969	7999.944754	13.690253	-0.058202	4.816007
283.913375	7999.972423	13.695258	-0.058234	4.816014
283.853571	7999.880517	13.700263	-0.058223	4.815988
283.783050	7999.901685	13.705267	-0.058210	4.815994
283.767163	7999.927052	13.710272	-0.058207	4.816002
283.875014	7999.914064	13.715277	-0.058227	4.815997
283.831868	7999.935730	13.720282	-0.058219	4.816004
283.783973	7999.929526	13.725287	-0.058210	4.816002
283.815948	7999.940804	13.730291	-0.058216	4.816005
283.947986	7999.985959	13.735296	-0.058241	4.816018
283.927537	7999.900112	13.740301	-0.058237	4.815993
283.975088	7999.959759	13.745306	-0.058246	4.816010
283.955425	7999.873926	13.750311	-0.058243	4.815985
284.038921	7999.888278	13.755315	-0.058258	4.815989
284.117327	7999.942074	13.760320	-0.058273	4.816004
284.076220	7999.912486	13.765325	-0.058266	4.815996
284.113828	8000.013627	13.770330	-0.058273	4.816025
284.022790	7999.975649	13.775335	-0.058256	4.816015
284.091144	7999.967286	13.780339	-0.058269	4.816012
283.930955	7999.985754	13.785344	-0.058239	4.816018
283.832373	7999.985040	13.790349	-0.058221	4.816018
283.996566	7999.952774	13.795354	-0.058251	4.816008
284.019476	7999.919007	13.800359	-0.058256	4.815998
283.930602	7999.988995	13.805363	-0.058239	4.816019
283.873003	7999.970861	13.810368	-0.058229	4.816014
284.024112	7999.971483	13.815373	-0.058257	4.816013
284.197680	7999.985337	13.820378	-0.058289	4.816016
284.108027	7999.933493	13.825383	-0.058273	4.816002
284.149436	7999.943874	13.830387	-0.058281	4.816005
284.129837	7999.996957	13.835392	-0.058277	4.816020
284.222019	7999.894992	13.840397	-0.058294	4.815990
284.040255	7999.939782	13.845402	-0.058261	4.816004
284.024903	7999.924553	13.850407	-0.058258	4.816000
283.984463	7999.914211	13.855411	-0.058250	4.815997
283.982476	7999.965477	13.860416	-0.058250	4.816012
284.072757	7999.994913	13.865421	-0.058267	4.816020
283.965537	7999.999385	13.870426	-0.058247	4.816022
283.727042	7999.927737	13.875431	-0.058203	4.816002
284.006646	7999.953136	13.880435	-0.058255	4.816008
284.153557	7999.963299	13.885440	-0.058283	4.816010
284.091235	7999.924775	13.890445	-0.058271	4.815999
284.041300	7999.984786	13.895450	-0.058262	4.816017
284.108801	7999.943282	13.900455	-0.058275	4.816005
284.019567	7999.966246	13.905459	-0.058258	4.816012
283.983951	7999.999803	13.910464	-0.058252	4.816022
284.112232	7999.898495	13.915469	-0.058275	4.815991
284.189545	7999.995016	13.920474	-0.058290	4.816019
283.936478	7999.955160	13.925479	-0.058243	4.816009
284.096053	7999.999747	13.930483	-0.058273	4.816021
284.080338	7999.983443	13.935488	-0.058270	4.816016
284.010916	7999.884951	13.940493	-0.058257	4.815988
283.958542	7999.975906	13.945498	-0.058248	4.816015
284.103252	7999.986029	13.950503	-0.058275	4.816017
284.173421	7999.930681	13.955507	-0.058288	4.816000
284.114287	7999.924273	13.960512	-0.058277	4.815999
284.189849	7999.922452	13.965517	-0.058291	4.815998
284.272780	8000.000909	13.970522	-0.058307	4.816020
283.851451	7999.868232	13.975527	-0.058228	4.815984
284.087816	7999.874679	13.980531	-0.058272	4.815985
284.079134	7999.930097	13.985536	-0.058271	4.816001
283.964613	7999.939779	13.990541	-0.058250	4.816004
284.223233	7999.987237	13.995546	-0.058298	4.816017
284.001493	7999.963980	14.000551	-0.058257	4.816011
284.018502	7999.969642	14.005555	-0.058260	4.816013
284.011485	7999.975937	14.010560	-0.058259	4.816015
284.043875	7999.906010	14.015565	-0.058265	4.815994
284.119680	7999.961897	14.020570	-0.058279	4.816010
284.026569	7999.924951	14.025575	-0.058262	4.816000
284.109744	7999.963875	14.030579	-0.058278	4.816010
284.192783	7999.958984	14.035584	-0.058293	4.816009
284.205948	7999.917559	14.040589	-0.058296	4.815996
284.047937	7999.987359	14.045594	-0.058266	4.816018
284.143850	7999.949577	14.050599	-0.058284	4.816006
284.268187	7999.949712	14.055603	-0.058308	4.816005
283.876341	7999.971446	14.060608	-0.058235	4.816014
283.988993	7999.874128	14.065613	-0.058256	4.815985
284.143595	7999.999837	14.070618	-0.058285	4.816021
284.170989	7999.965083	14.075623	-0.058290	4.816010
284.319972	7999.929335	14.080627	-0.058318	4.815999
284.256849	7999.932471	14.085632	-0.058306	4.816000
284.023163	7999.886557	14.090637	-0.058263	4.815988
284.070205	7999.919480	14.095642	-0.058272	4.815998
284.081682	7999.911151	14.100647	-0.058274	4.815995
284.366436	7999.894969	14.105651	-0.058327	4.815989
284.090885	7999.991482	14.110656	-0.058276	4.816019
284.078680	7999.945322	14.115661	-0.058274	4.816005
284.062936	7999.997406	14.120666	-0.058271	4.816020
283.931844	7999.943741	14.125671	-0.058246	4.816005
283.978028	7999.944591	14.130675	-0.058255	4.816005
284.093222	7999.967000	14.135680	-0.058277	4.816011
283.986856	7999.899893	14.140685	-0.058257	4.815992
284.082058	7999.960406	14.145690	-0.058275	4.816010
284.318752	7999.970066	14.150695	-0.058319	4.816011
284.479898	7999.924921	14.155699	-0.058349	4.815997
284.162215	7999.955485	14.160704	-0.058290	4.816008
284.206839	7999.870820	14.165709	-0.058298	4.815983
284.364078	7999.983755	14.170714	-0.058328	4.816015
284.118559	7999.890607	14.175719	-0.058282	4.815989
284.016848	7999.975322	14.180723	-0.058263	4.816014
284.110625	8000.001616	14.185728	-0.058281	4.816021
284.159777	7999.962983	14.190733	-0.058290	4.816010
284.029396	8000.005502	14.195738	-0.058266	4.816023
284.049915	7999.958869	14.200743	-0.058270	4.816009
284.139193	7999.923103	14.205747	-0.058287	4.815998
284.294883	7999.969757	14.210752	-0.058316	4.816011
284.174213	7999.947270	14.215757	-0.058294	4.816005
284.235727	7999.962291	14.220762	-0.058305	4.816009
284.106251	7999.940711	14.225767	-0.058281	4.816004
284.130704	7999.975361	14.230771	-0.058286	4.816014
284.200592	8000.007632	14.235776	-0.058299	4.816023
284.061016	7999.930303	14.240781	-0.058273	4.816001
284.093077	8000.014246	14.245786	-0.058279	4.816025
284.179679	8000.001940	14.250791	-0.058295	4.816021
284.318925	7999.956397	14.255795	-0.058321	4.816007
284.248242	7999.679430	14.260800	-0.058308	4.815926

283.981134	7996.300419	14.265805	-0.058256	4.814941
284.052750	7990.801755	14.270810	-0.058266	4.813333
283.885812	7983.960847	14.275815	-0.058231	4.811334
284.005819	7976.642384	14.280819	-0.058248	4.809192
284.132110	7969.017947	14.285824	-0.058267	4.806960
284.102845	7961.181118	14.290829	-0.058257	4.804666
283.930070	7953.410601	14.295834	-0.058219	4.802391
283.862843	7945.371908	14.300839	-0.058202	4.800035
284.006694	7937.453549	14.305843	-0.058224	4.797713
283.835046	7929.450791	14.310848	-0.058186	4.795366
283.751869	7921.403482	14.315853	-0.058166	4.793004
284.053087	7913.404625	14.320858	-0.058217	4.790654
283.821923	7905.414943	14.325863	-0.058169	4.788308
283.733847	7897.419838	14.330867	-0.058147	4.785958
283.601028	7889.446051	14.335872	-0.058117	4.783614
283.675729	7881.404087	14.340877	-0.058126	4.781248
283.557606	7873.468144	14.345882	-0.058099	4.778912
283.443663	7865.378288	14.350887	-0.058073	4.776530
283.509432	7857.388378	14.355891	-0.058080	4.774175
283.390452	7849.360539	14.360896	-0.058053	4.771809
283.307764	7841.375350	14.365901	-0.058032	4.769454
283.393505	7833.390179	14.370906	-0.058043	4.767097
283.430610	7825.378654	14.375911	-0.058045	4.764732
283.284164	7817.458395	14.380915	-0.058012	4.762393
283.263156	7809.403328	14.385920	-0.058003	4.760012
283.194737	7801.450898	14.390925	-0.057986	4.757661
283.075920	7793.376221	14.395930	-0.057958	4.755273
282.906082	7785.342957	14.400935	-0.057921	4.752896
283.038717	7777.328183	14.405939	-0.057941	4.750522
282.866666	7769.328296	14.410944	-0.057904	4.748152
282.639151	7761.313891	14.415949	-0.057856	4.745777
282.798971	7753.384079	14.420954	-0.057881	4.743425
282.707432	7745.360470	14.425959	-0.057859	4.741044
282.658855	7737.367725	14.430963	-0.057845	4.738672
282.712520	7729.340263	14.435968	-0.057850	4.736287
282.695747	7721.332834	14.440973	-0.057841	4.733907
282.554198	7713.300757	14.445978	-0.057810	4.731520
282.385108	7705.308168	14.450983	-0.057773	4.729143
282.519355	7697.327142	14.455987	-0.057793	4.726767
282.442850	7689.326887	14.460992	-0.057774	4.724385
282.400613	7681.341538	14.465997	-0.057761	4.722006
282.530434	7673.307547	14.471002	-0.057780	4.719611
282.258839	7665.364622	14.476007	-0.057724	4.717242
282.212411	7657.311901	14.481011	-0.057711	4.714840
282.143001	7649.320592	14.486016	-0.057693	4.712454
282.232657	7641.264852	14.491021	-0.057704	4.710048
282.316566	7633.361460	14.496026	-0.057715	4.707686
282.238810	7625.262206	14.501031	-0.057695	4.705264
282.302466	7617.352044	14.506035	-0.057702	4.702898
282.345673	7609.311144	14.511040	-0.057705	4.700491
282.032609	7601.315118	14.516045	-0.057641	4.698097
282.103362	7593.330635	14.521050	-0.057649	4.695705
282.008131	7585.336367	14.526055	-0.057627	4.693309
282.046430	7577.230721	14.531059	-0.057629	4.690878
282.135473	7569.320009	14.536064	-0.057640	4.688504
281.936876	7561.299886	14.541069	-0.057598	4.686096
282.108314	7553.299133	14.546074	-0.057625	4.683693
281.931272	7545.272957	14.551079	-0.057587	4.681281
281.995372	7537.348155	14.556083	-0.057594	4.678898
281.970848	7529.309543	14.561088	-0.057584	4.676480
281.582158	7521.176305	14.566093	-0.057506	4.674032
281.821757	7513.185142	14.571098	-0.057546	4.671625
281.618351	7505.176662	14.576103	-0.057503	4.669213
281.713194	7497.203161	14.581107	-0.057515	4.666809
281.674627	7489.224700	14.586112	-0.057503	4.664402
281.701796	7481.290043	14.591117	-0.057503	4.662008
281.659289	7473.224706	14.596122	-0.057490	4.659573
281.249534	7465.264011	14.601127	-0.057409	4.657168
281.304243	7457.237601	14.606131	-0.057414	4.654742
281.335112	7449.263759	14.611136	-0.057414	4.652331
281.165738	7441.165225	14.616141	-0.057378	4.649881
281.265149	7433.263970	14.621146	-0.057391	4.647489
281.185929	7425.223805	14.626151	-0.057371	4.645053
281.186805	7417.286057	14.631155	-0.057366	4.642648
281.260629	7409.225059	14.636160	-0.057375	4.640204
281.217431	7401.245035	14.641165	-0.057362	4.637783
281.228565	7393.250876	14.646170	-0.057359	4.635356
281.129575	7385.192724	14.651175	-0.057335	4.632909
280.913953	7377.148801	14.656179	-0.057290	4.630465
280.983769	7369.230135	14.661184	-0.057298	4.628058
280.834298	7361.178524	14.666189	-0.057265	4.625609
280.748127	7353.238057	14.671194	-0.057244	4.623193
280.794502	7345.197520	14.676199	-0.057247	4.620744
280.768951	7337.243051	14.681203	-0.057238	4.618321
280.604874	7329.195247	14.686208	-0.057202	4.615868
280.430552	7321.185550	14.691213	-0.057164	4.613426
280.503020	7313.175407	14.696218	-0.057173	4.610981
280.253236	7305.205901	14.701223	-0.057121	4.608548
280.239584	7297.160231	14.706227	-0.057113	4.606091
280.536814	7289.185508	14.711232	-0.057164	4.603653
280.307769	7281.144137	14.716237	-0.057116	4.601195
280.434393	7273.222598	14.721242	-0.057134	4.598771
280.324647	7265.183800	14.726247	-0.057109	4.596310
280.317732	7257.166688	14.731251	-0.057102	4.593855
280.170410	7249.144727	14.736256	-0.057070	4.591396
280.239017	7241.114839	14.741261	-0.057078	4.588934
280.179066	7233.115764	14.746266	-0.057061	4.586481
279.820139	7225.146643	14.751271	-0.056989	4.584034
279.948252	7217.159112	14.756275	-0.057008	4.581581
279.997386	7209.168796	14.761280	-0.057012	4.579126
279.772939	7201.153673	14.766285	-0.056965	4.576662
279.855859	7193.158732	14.771290	-0.056976	4.574203
279.833446	7185.093201	14.776295	-0.056966	4.571721
279.841046	7177.090799	14.781299	-0.056963	4.569256
279.653489	7169.112376	14.786304	-0.056923	4.566798
279.799981	7161.098077	14.791309	-0.056945	4.564328
279.783758	7153.180559	14.796314	-0.056937	4.561886
279.492060	7145.157794	14.801319	-0.056877	4.559410
279.334500	7137.179556	14.806323	-0.056843	4.556946
279.567719	7129.139842	14.811328	-0.056881	4.554462
279.549470	7121.074961	14.816333	-0.056872	4.551970
279.449858	7113.082410	14.821338	-0.056849	4.549498
279.391718	7105.112255	14.826343	-0.056833	4.547031
279.309218	7097.118322	14.831347	-0.056812	4.544556
279.357001	7089.169566	14.836352	-0.056816	4.542094
279.129652	7081.100406	14.841357	-0.056769	4.539592
279.160136	7073.176551	14.846362	-0.056769	4.537135
279.024732	7065.133026	14.851367	-0.056739	4.534639
279.131511	7057.087794	14.856371	-0.056754	4.532141
279.224429	7049.088228	14.861376	-0.056766	4.529657
279.061173	7041.105408	14.866381	-0.056731	4.527175
279.057849	7033.125166	14.871386	-0.056725	4.524694
278.934170	7025.160019	14.876391	-0.056697	4.522215
278.935528	7017.129394	14.881395	-0.056692	4.519715
278.807266	7009.186161	14.886400	-0.056663	4.517240
278.588320	7001.088673	14.891405	-0.056617	4.514716
278.552140	6993.034675	14.896410	-0.056605	4.512205
278.341439	6985.029348	14.901415	-0.056561	4.509706
278.292773	6977.039445	14.906419	-0.056547	4.507212
278.527104	6969.034029	14.911424	-0.056585	4.504712
278.356308	6961.079823	14.916429	-0.056548	4.502225
278.511352	6953.144651	14.921434	-0.056572	4.499744
278.251415	6945.127166	14.926439	-0.056518	4.497235
278.309023	6937.050984	14.931443	-0.056524	4.494707
278.317441	6929.069401	14.936448	-0.056521	4.492207
278.286386	6921.032836	14.941453	-0.056510	4.489688
278.231759	6913.114463	14.946458	-0.056494	4.487205
278.165215	6905.045425	14.951463	-0.056477	4.484673
278.208980	6897.084402	14.956467	-0.056480	4.482174
278.084570	6889.073671	14.961472	-0.056452	4.479657
277.973143	6881.073338	14.966477	-0.056426	4.477142
277.884069	6873.086277	14.971482	-0.056404	4.474630
278.110895	6865.009476	14.976487	-0.056441	4.472090
278.099442	6856.994026	14.981491	-0.056434	4.469566
278.036545	6849.028212	14.986496	-0.056417	4.467057
277.936596	6841.034604	14.991501	-0.056393	4.464537
278.151328	6833.067055	14.996506	-0.056428	4.462025
278.003399	6825.031560	15.001511	-0.056396	4.459489
277.812575	6817.043671	15.006515	-0.056355	4.456966
277.884760	6809.031835	15.011520	-0.056363	4.454436
277.904034	6801.002407	15.016525	-0.056362	4.451898
277.713784	6793.022359	15.021530	-0.056321	4.449373
277.679108	6785.017519	15.026535	-0.056310	4.446840
277.710551	6777.029306	15.031539	-0.056310	4.444311
277.498893	6769.050492	15.036544	-0.056266	4.441783
277.495063	6761.027528	15.041549	-0.056260	4.439239
277.675929	6753.050206	15.046554	-0.056289	4.436710
277.426125	6745.011922	15.051559	-0.056237	4.434158
277.267993	6736.957555	15.056563	-0.056203	4.431600
277.380206	6728.984006	15.061568	-0.056218	4.429067
277.427160	6720.957909	15.066573	-0.056222	4.426516
277.360245	6713.032132	15.071578	-0.056204	4.423994
277.113709	6704.995642	15.076583	-0.056153	4.421436
277.149655	6696.993384	15.081587	-0.056155	4.418887
277.012138	6688.992256	15.086592	-0.056124	4.416337
276.901049	6680.977821	15.091597	-0.056098	4.413782
277.199071	6672.978897	15.096602	-0.056149	4.411231
277.006304	6664.976893	15.101607	-0.056108	4.408676
276.831103	6657.008674	15.106611	-0.056070	4.406131
276.722686	6649.039266	15.111616	-0.056045	4.403583
276.691373	6640.971849	15.116621	-0.056034	4.401004
276.641778	6633.007989	15.121626	-0.056020	4.398455
276.355199	6624.982221	15.126631	-0.055961	4.395885
276.646363	6616.989294	15.131635	-0.056010	4.393326
276.745392	6608.942596	15.136640	-0.056023	4.390747
276.501148	6600.984910	15.141645	-0.055973	4.388194
276.376321	6592.965834	15.146650	-0.055945	4.385621
276.403008	6584.996676	15.151655	-0.055944	4.383062
276.302702	6576.970150	15.156659	-0.055921	4.380483
276.294218	6568.989583	15.161664	-0.055914	4.377918
276.247951	6560.958064	15.166669	-0.055900	4.375334
276.282955	6553.015264	15.171674	-0.055902	4.372778
276.061250	6544.972999	15.176679	-0.055855	4.370187
276.116305	6537.019864	15.181683	-0.055860	4.367625
276.179433	6528.968621	15.186688	-0.055867	4.365030
276.134150	6521.022779	15.191693	-0.055854	4.362466
276.223022	6513.033755	15.196698	-0.055865	4.359888
276.157560	6505.052257	15.201703	-0.055848	4.357310
275.892975	6496.985520	15.206707	-0.055793	4.354701
275.619150	6488.916183	15.211712	-0.055737	4.352091
275.548380	6480.894270	15.216717	-0.055719	4.349495
275.666358	6472.942989	15.221722	-0.055736	4.346921
275.636882	6464.934669	15.226727	-0.055725	4.344327
275.690711	6456.995007	15.231731	-0.055730	4.341754
275.663942	6449.006771	15.236736	-0.055720	4.339163
275.592475	6440.944388	15.241741	-0.055702	4.336546
275.757656	6432.972508	15.246746	-0.055727	4.333958
275.497504	6424.926538	15.251751	-0.055674	4.331342
275.465842	6416.958626	15.256755	-0.055663	4.328752
275.343202	6408.973398	15.261760	-0.055635	4.326153
275.296983	6400.973213	15.266765	-0.055621	4.323549
275.425981	6392.964603	15.271770	-0.055640	4.320941
275.226301	6384.991709	15.276775	-0.055598	4.318342
275.156673	6376.928077	15.281779	-0.055580	4.315712
275.225179	6368.941972	15.286784	-0.055587	4.313106
275.017052	6360.912224	15.291789	-0.055543	4.310483
275.091388	6352.922314	15.296794	-0.055552	4.307874
275.119175	6344.922981	15.301799	-0.055552	4.305259
274.982125	6336.953192	15.306803	-0.055522	4.302651
274.912243	6328.954356	15.311808	-0.055503	4.300033
275.018285	6320.940214	15.316813	-0.055518	4.297409
275.232836	6312.912244	15.321818	-0.055553	4.294780
275.152094	6304.902624	15.326823	-0.055533	4.292153
274.946310	6296.952242	15.331827	-0.055489	4.289543
274.799234	6288.927448	15.336832	-0.055457	4.286907
274.809773	6280.916259	15.341837	-0.055454	4.284276
274.672470	6272.913541	15.346842	-0.055423	4.281644
274.711321	6264.957096	15.351847	-0.055425	4.279028
274.582589	6256.923295	15.356851	-0.055396	4.276383
274.456881	6248.931412	15.361856	-0.055368	4.273750
274.347871	6240.884427	15.366861	-0.055342	4.271098
274.424973	6232.897482	15.371866	-0.055351	4.268465
274.365817	6224.873461	15.376871	-0.055335	4.265817
274.292929	6216.865202	15.381875	-0.055317	4.263173
274.558621	6208.904320	15.386880	-0.055361	4.260545
274.530469	6200.914266	15.391885	-0.055351	4.257904
274.311443	6192.936969	15.396890	-0.055305	4.255264
274.312839	6184.903321	15.401895	-0.055300	4.252605
274.457109	6176.865287	15.406899	-0.055322	4.249945
274.174247	6168.945287	15.411904	-0.055264	4.247318
273.990728	6160.853516	15.416909	-0.055225	4.244633
274.143384	6152.927225	15.421914	-0.055248	4.242005
273.954434	6144.920100	15.426919	-0.055208	4.239345
273.786842	6136.963539	15.431923	-0.055171	4.236700
274.120773	6128.922178	15.436928	-0.055228	4.234030
273.879103	6120.925159	15.441933	-0.055178	4.231368
273.810541	6112.923763	15.446938	-0.055160	4.228704
273.630705	6104.917449	15.451943	-0.055122	4.226036
273.767028	6096.926999	15.456947	-0.055142	4.223375
273.513967	6088.913316	15.461952	-0.055090	4.220700
273.475700	6080.961333	15.466957	-0.055078	4.218046
273.598837	6072.943351	15.471962	-0.055095	4.215371
273.382387	6064.933747	15.476967	-0.055050	4.212692
273.288789	6056.869724	15.481971	-0.055027	4.209996
273.341205	6048.944693	15.486976	-0.055032	4.207345
273.471354	6040.899264	15.491981	-0.055051	4.204653
273.505044	6032.987611	15.496986	-0.055053	4.202004
273.413143	6024.977626	15.501991	-0.055030	4.199318
273.456299	6016.951046	15.506995	-0.055033	4.196627
273.291424	6008.907105	15.512000	-0.054997	4.193925
272.986823	6000.805785	15.517005	-0.054935	4.191202
273.316900	5992.900209	15.522010	-0.054992	4.188549
273.163566	5984.859498	15.527015	-0.054958	4.185844
273.028217	5976.912543	15.532019	-0.054928	4.183168
273.121497	5968.929256	15.537024	-0.054940	4.180482
272.961705	5960.884956	15.542029	-0.054905	4.177770
272.824351	5952.889676	15.547034	-0.054875	4.175073
272.801111	5944.903377	15.552039	-0.054865	4.172379
272.910488	5936.856963	15.557043	-0.054880	4.169664
272.746031	5928.932725	15.562048	-0.054845	4.166985
272.619152	5920.871154	15.567053	-0.054816	4.164259
272.641641	5912.933680	15.572058	-0.054815	4.161575
272.539469	5904.939037	15.577063	-0.054791	4.158868
272.573831	5896.895356	15.582067	-0.054792	4.156145
272.724521	5888.901872	15.587072	-0.054815	4.153437
272.595732	5880.869540	15.592077	-0.054786	4.150712
272.301474	5872.882160	15.597082	-0.054726	4.147999
272.132950	5864.870131	15.602087	-0.054690	4.145276
272.186897	5856.911879	15.607091	-0.054695	4.142573
272.317225	5848.897436	15.612096	-0.054714	4.139850
271.915237	5840.918527	15.617101	-0.054634	4.137130
272.212998	5832.904236	15.622106	-0.054684	4.134405
272.029959	5824.862432	15.627111	-0.054645	4.131664
271.947203	5816.882037	15.632115	-0.054625	4.128942
271.905866	5808.878949	15.637120	-0.054612	4.126212
272.109860	5800.880702	15.642125	-0.054645	4.123484
271.892247	5792.919168	15.647130	-0.054599	4.120762
271.704482	5784.925398	15.652135	-0.054559	4.118027
271.838520	5776.861533	15.657139	-0.054579	4.115271
271.744080	5768.880617	15.662144	-0.054556	4.112538
271.654507	5760.849287	15.667149	-0.054534	4.109787
271.525497	5752.894947	15.672154	-0.054505	4.107059
271.586047	5744.861609	15.677159	-0.054511	4.104305
271.364430	5736.891395	15.682163	-0.054465	4.101567
271.430700	5728.930416	15.687168	-0.054472	4.098834
271.338623	5720.880755	15.692173	-0.054450	4.096066
271.354724	5712.919635	15.697178	-0.054448	4.093329
271.116653	5704.897275	15.702183	-0.054398	4.090565
271.321786	5696.895303	15.707187	-0.054431	4.087813
271.380341	5688.900626	15.712192	-0.054437	4.085059
271.204815	5680.942949	15.717197	-0.054400	4.082313
271.286814	5672.949099	15.722202	-0.054410	4.079556
271.152127	5664.962711	15.727207	-0.054380	4.076796
271.004207	5656.924499	15.732211	-0.054347	4.074017
270.980854	5648.925771	15.737216	-0.054337	4.071251
270.897705	5640.907791	15.742221	-0.054317	4.068476
271.045958	5632.906891	15.747226	-0.054339	4.065708
270.879397	5624.940130	15.752231	-0.054303	4.062946
270.962306	5616.895969	15.757235	-0.054313	4.060158
271.071535	5608.974095	15.762240	-0.054329	4.057412
270.948760	5600.907795	15.767245	-0.054301	4.054610
271.099333	5592.917788	15.772250	-0.054324	4.051836
270.770484	5584.932995	15.777255	-0.054257	4.049056
270.775180	5576.906971	15.782259	-0.054253	4.046263
270.716622	5568.959024	15.787264	-0.054237	4.043496
270.447142	5560.935686	15.792269	-0.054182	4.040697
270.460812	5552.958185	15.797274	-0.054179	4.037916
270.307080	5544.941281	15.802279	-0.054146	4.035117
270.259638	5536.826316	15.807283	-0.054132	4.032284
270.443927	5528.859193	15.812288	-0.054161	4.029503
270.367195	5520.879089	15.817293	-0.054141	4.026713
270.363467	5512.894313	15.822298	-0.054136	4.023919
270.501446	5504.894772	15.827303	-0.054156	4.021121
270.295844	5496.929750	15.832307	-0.054113	4.018328
270.250343	5488.918942	15.837312	-0.054099	4.015519
270.175631	5480.907913	15.842317	-0.054080	4.012708
270.253791	5472.880772	15.847322	-0.054090	4.009891
270.077593	5464.950320	15.852327	-0.054052	4.007102
270.048680	5456.885834	15.857331	-0.054041	4.004267
270.097634	5448.946962	15.862336	-0.054045	4.001475
269.978139	5440.901394	15.867341	-0.054018	3.998641
269.883186	5432.925168	15.872346	-0.053995	3.995829
269.936935	5424.888644	15.877351	-0.054000	3.992997
269.805824	5416.868757	15.882355	-0.053970	3.990166
269.650661	5408.938806	15.887360	-0.053937	3.987364
269.661332	5400.897454	15.892365	-0.053933	3.984523
269.907333	5392.933238	15.897370	-0.053974	3.981711
269.777723	5384.933478	15.902375	-0.053945	3.978879
269.619916	5376.913442	15.907379	-0.053910	3.976037
269.570766	5368.904782	15.912384	-0.053896	3.973199
269.456733	5360.870543	15.917389	-0.053870	3.970349
269.525555	5352.951505	15.922394	-0.053877	3.967540
269.548561	5344.940863	15.927399	-0.053877	3.964696
269.463540	5336.978793	15.932403	-0.053856	3.961866
269.386355	5328.993123	15.937408	-0.053836	3.959025
269.243804	5320.985613	15.942413	-0.053805	3.956173
269.204751	5312.958878	15.947418	-0.053792	3.953315
269.266209	5304.913044	15.952423	-0.053799	3.950449
269.143576	5296.933465	15.957427	-0.053771	3.947601
269.277626	5288.956128	15.962432	-0.053790	3.944757
269.081575	5280.956708	15.967437	-0.053749	3.941896
268.915700	5272.988795	15.972442	-0.053713	3.939046
269.071228	5264.990169	15.977447	-0.053737	3.936188
269.046970	5256.958101	15.982451	-0.053727	3.933313
268.744048	5248.976070	15.987456	-0.053666	3.930449
268.604678	5240.987596	15.992461	-0.053635	3.927583
268.679167	5232.998813	15.997466	-0.053643	3.924719
268.567134	5225.029427	16.002471	-0.053617	3.921857
268.421845	5217.025866	16.007475	-0.053585	3.918979
268.634535	5208.998217	16.012480	-0.053620	3.916097
268.700431	5200.956861	16.017485	-0.053627	3.913206
268.685327	5192.974051	16.022490	-0.053619	3.910331
268.595465	5185.002633	16.027495	-0.053597	3.907458
268.389731	5176.970291	16.032499	-0.053554	3.904558
268.380733	5168.994540	16.037504	-0.053547	3.901680
268.154835	5161.004657	16.042509	-0.053500	3.898791
268.280517	5153.007939	16.047514	-0.053518	3.895904
268.073029	5144.990250	16.052519	-0.053474	3.893001
267.965332	5136.942432	16.057523	-0.053449	3.890087
268.136019	5129.021541	16.062528	-0.053476	3.887221
268.121879	5120.965361	16.067533	-0.053468	3.884301
267.900531	5112.985459	16.072538	-0.053422	3.881403
267.957008	5105.030569	16.077543	-0.053427	3.878516
267.963780	5097.002580	16.082547	-0.053423	3.875600
267.790305	5088.810741	16.087552	-0.053386	3.872619
267.707051	5080.815235	16.092557	-0.053365	3.869709
267.815499	5072.891864	16.097562	-0.053380	3.866826
267.629744	5064.930132	16.102567	-0.053341	3.863922
267.682710	5056.945401	16.107571	-0.053345	3.861012
267.618110	5048.994386	16.112576	-0.053328	3.858109
267.552629	5040.973376	16.117581	-0.053311	3.855179
267.340842	5033.009135	16.122586	-0.053266	3.852264
267.358740	5024.968542	16.127591	-0.053265	3.849324
267.369628	5016.984782	16.132595	-0.053262	3.846402
267.444003	5008.990829	16.137600	-0.053270	3.843475
267.250187	5001.011737	16.142605	-0.053229	3.840547
267.335076	4993.045550	16.147610	-0.053240	3.837626
267.159978	4985.047951	16.152615	-0.053202	3.834686
267.037736	4977.023898	16.157619	-0.053174	3.831736
267.182700	4969.034460	16.162624	-0.053196	3.828801
267.105994	4961.024492	16.167629	-0.053177	3.825852
267.045372	4953.067293	16.172634	-0.053160	3.822920
266.918066	4945.045473	16.177639	-0.053132	3.819961
266.936278	4937.072465	16.182643	-0.053130	3.817021
267.030999	4929.074198	16.187648	-0.053142	3.814071
266.936944	4921.050601	16.192653	-0.053120	3.811105
266.951073	4913.054124	16.197658	-0.053117	3.808149
267.003865	4905.059109	16.202663	-0.053122	3.805192
266.844446	4897.110320	16.207667	-0.053087	3.802246
266.766483	4889.107480	16.212672	-0.053068	3.799278
266.610390	4881.091896	16.217677	-0.053034	3.796303
266.478189	4873.083806	16.222682	-0.053004	3.793328
266.462698	4865.039124	16.227687	-0.052996	3.790339
266.656129	4857.042300	16.232691	-0.053027	3.787371
266.637015	4849.067507	16.237696	-0.053018	3.784404
266.199024	4841.090138	16.242701	-0.052931	3.781424
266.402036	4833.088056	16.247706	-0.052964	3.778447
266.567500	4825.080198	16.252711	-0.052990	3.775464
266.270781	4817.055099	16.257715	-0.052929	3.772463
266.058664	4809.125054	16.262720	-0.052885	3.769496
266.028057	4801.072757	16.267725	-0.052874	3.766486
266.105387	4793.095511	16.272730	-0.052883	3.763503
266.212594	4785.077747	16.277735	-0.052898	3.760504
265.931618	4777.113141	16.282739	-0.052841	3.757514
265.982267	4769.139042	16.287744	-0.052845	3.754525
265.875767	4761.078561	16.292749	-0.052820	3.751497
266.049454	4753.078984	16.297754	-0.052847	3.748497
265.943782	4745.088746	16.302759	-0.052823	3.745491
265.720073	4737.117206	16.307763	-0.052776	3.742487
265.780041	4729.152915	16.312768	-0.052782	3.739490
265.635058	4721.136440	16.317773	-0.052750	3.736466
265.694791	4713.112166	16.322778	-0.052756	3.733441
265.403264	4705.115412	16.327783	-0.052696	3.730416
265.428062	4697.117095	16.332787	-0.052696	3.727396
265.761725	4689.122420	16.337792	-0.052753	3.724381
265.559329	4681.161984	16.342797	-0.052710	3.721365
265.524159	4673.163766	16.347802	-0.052699	3.718335
265.471275	4665.181443	16.352807	-0.052684	3.715309
265.439352	4657.078429	16.357811	-0.052672	3.712235
265.353609	4649.105606	16.362816	-0.052651	3.709207
265.419091	4641.092721	16.367821	-0.052659	3.706165
265.243239	4633.175713	16.372826	-0.052621	3.703150
265.053865	4625.177526	16.377831	-0.052580	3.700102
264.901978	4617.187704	16.382835	-0.052547	3.697056
264.969353	4609.195292	16.387840	-0.052554	3.694011
264.735221	4601.162712	16.392845	-0.052506	3.690941
265.052751	4593.189360	16.397850	-0.052560	3.687905
265.003291	4585.194085	16.402855	-0.052545	3.684849
265.001983	4577.221909	16.407859	-0.052540	3.681801
264.894330	4569.251084	16.412864	-0.052515	3.678747
264.777901	4561.235366	16.417869	-0.052488	3.675674
264.677791	4553.220449	16.422874	-0.052464	3.672599
264.602676	4545.204950	16.427879	-0.052445	3.669521
264.627184	4537.199356	16.432883	-0.052445	3.666448
264.797262	4529.235443	16.437888	-0.052471	3.663391
264.452178	4521.241091	16.442893	-0.052402	3.660307
264.261687	4513.270040	16.447898	-0.052361	3.657234
264.561649	4505.225884	16.452903	-0.052412	3.654142
264.397329	4497.225327	16.457907	-0.052376	3.651053
264.322621	4489.250637	16.462912	-0.052357	3.647973
264.346634	4481.184748	16.467917	-0.052357	3.644858
264.467870	4473.283004	16.472922	-0.052374	3.641806
264.415819	4465.272209	16.477927	-0.052359	3.638705
264.156744	4457.292886	16.482931	-0.052306	3.635608
264.184701	4449.275063	16.487936	-0.052306	3.632501
263.896443	4441.235133	16.492941	-0.052247	3.629374
263.865897	4433.248010	16.497946	-0.052237	3.626272
263.864814	4425.271327	16.502951	-0.052231	3.623172
263.712896	4417.275017	16.507955	-0.052198	3.620058
263.869615	4409.310718	16.512960	-0.052222	3.616962
263.746890	4401.259705	16.517965	-0.052194	3.613822
263.845051	4393.266742	16.522970	-0.052207	3.610708
263.614441	4385.313261	16.527975	-0.052159	3.607597
263.477834	4377.284253	16.532979	-0.052129	3.604457
263.590053	4369.361316	16.537984	-0.052144	3.601362
263.545848	4361.346935	16.542989	-0.052131	3.598225
263.552344	4353.345541	16.547994	-0.052127	3.595092
263.606649	4345.374798	16.552999	-0.052132	3.591969
263.438789	4337.337704	16.558003	-0.052096	3.588811
263.401415	4329.362819	16.563008	-0.052084	3.585678
263.173212	4321.372860	16.568013	-0.052036	3.582531
263.147615	4313.371515	16.573018	-0.052026	3.579383
263.184905	4305.404403	16.578023	-0.052028	3.576248
263.042477	4297.361423	16.583027	-0.051997	3.573074
263.167362	4289.368020	16.588032	-0.052015	3.569925
263.177060	4281.394724	16.593037	-0.052011	3.566778
262.999534	4273.409710	16.598042	-0.051973	3.563617
263.049660	4265.412885	16.603047	-0.051978	3.560456
263.044037	4257.453241	16.608051	-0.051971	3.557306
262.930962	4249.414805	16.613056	-0.051945	3.554118
262.859633	4241.320757	16.618061	-0.051927	3.550906
262.885325	4233.336204	16.623066	-0.051926	3.547738
262.752913	4225.358687	16.628071	-0.051897	3.544565
262.566872	4217.426103	16.633075	-0.051857	3.541406
262.599250	4209.432696	16.638080	-0.051858	3.538226
262.499966	4201.421025	16.643085	-0.051834	3.535031
262.584960	4193.409920	16.648090	-0.051845	3.531840
262.616539	4185.420190	16.653095	-0.051846	3.528653
262.401493	4177.443695	16.658099	-0.051801	3.525461
262.372471	4169.500329	16.663104	-0.051790	3.522284
262.207627	4161.484714	16.668109	-0.051754	3.519072
262.377319	4153.473769	16.673114	-0.051781	3.515869
262.277143	4145.470294	16.678119	-0.051757	3.512658
261.980692	4137.488348	16.683123	-0.051697	3.509446
262.152926	4129.469546	16.688128	-0.051724	3.506231
261.905858	4121.532794	16.693133	-0.051673	3.503033
261.802082	4113.524941	16.698138	-0.051648	3.499808
261.845670	4105.547290	16.703143	-0.051651	3.496597
261.728685	4097.518102	16.708147	-0.051624	3.493357
261.847595	4089.517643	16.713152	-0.051641	3.490133
261.738982	4081.559152	16.718157	-0.051616	3.486915
261.893174	4073.538242	16.723162	-0.051640	3.483678
261.840218	4065.576329	16.728167	-0.051625	3.480455
261.593103	4057.593049	16.733171	-0.051574	3.477215
261.703166	4049.597854	16.738176	-0.051589	3.473978
261.460712	4041.577720	16.743181	-0.051539	3.470716
261.274906	4033.563095	16.748186	-0.051499	3.467455
261.389148	4025.586187	16.753191	-0.051515	3.464217
261.386973	4017.614385	16.758195	-0.051510	3.460973
261.550451	4009.620083	16.763200	-0.051535	3.457723
261.289925	4001.628619	16.768205	-0.051482	3.454457
261.234060	3993.577305	16.773210	-0.051466	3.451170
261.386101	3985.601914	16.778215	-0.051489	3.447918
261.147084	3977.610302	16.783219	-0.051440	3.444643
261.094244	3969.660285	16.788224	-0.051425	3.441389
261.087875	3961.674464	16.793229	-0.051418	3.438118
260.917025	3953.645565	16.798234	-0.051381	3.434820
260.905816	3945.642743	16.803239	-0.051374	3.431536
260.844083	3937.628892	16.808243	-0.051358	3.428242
260.820427	3929.649287	16.813248	-0.051348	3.424961
260.916830	3921.694115	16.818253	-0.051361	3.421690
260.685919	3913.699724	16.823258	-0.051313	3.418389
260.752156	3905.703254	16.828263	-0.051320	3.415094
260.505152	3897.687976	16.833267	-0.051269	3.411778
260.614213	3889.717078	16.838272	-0.051284	3.408489
260.532668	3881.704627	16.843277	-0.051264	3.405172
260.565759	3873.747102	16.848282	-0.051265	3.401880
260.674543	3865.780466	16.853287	-0.051280	3.398582
260.544116	3857.781910	16.858291	-0.051251	3.395261
260.499956	3849.724698	16.863296	-0.051237	3.391914
260.070043	3841.715109	16.868301	-0.051152	3.388571
260.061886	3833.715922	16.873306	-0.051146	3.385243
260.397513	3825.766280	16.878311	-0.051203	3.381945
260.181250	3817.778452	16.883315	-0.051158	3.378608
260.023266	3809.816159	16.888320	-0.051123	3.375280
259.903029	3801.803322	16.893325	-0.051096	3.371930
259.855092	3793.807333	16.898330	-0.051082	3.368586
259.713264	3785.832481	16.903335	-0.051050	3.365244
259.744293	3777.827858	16.908339	-0.051051	3.361892
259.777797	3769.857046	16.913344	-0.051052	3.358551
259.672524	3761.857659	16.918349	-0.051027	3.355190
259.795865	3753.826009	16.923354	-0.051045	3.351820
259.757461	3745.845916	16.928359	-0.051033	3.348462
259.688227	3737.826832	16.933363	-0.051015	3.345084
259.576598	3729.921721	16.938368	-0.050989	3.341749
259.860043	3721.881009	16.943373	-0.051037	3.338367
259.744494	3713.898315	16.948378	-0.051010	3.334993
259.578029	3705.934077	16.953383	-0.050974	3.331620
259.539170	3697.904222	16.958387	-0.050962	3.328221
259.585500	3689.914226	16.963392	-0.050965	3.324839
259.416848	3681.968755	16.968397	-0.050929	3.321464
259.419477	3673.971625	16.973402	-0.050924	3.318070
259.389227	3666.004656	16.978407	-0.050913	3.314684
259.204623	3657.961077	16.983411	-0.050874	3.311257
259.043807	3649.984664	16.988416	-0.050839	3.307855
258.973849	3641.970449	16.993421	-0.050821	3.304437
258.938089	3633.990800	16.998426	-0.050809	3.301031
259.045343	3626.034506	17.003431	-0.050824	3.297638
258.864165	3618.037504	17.008435	-0.050785	3.294212
258.933360	3609.996741	17.013440	-0.050793	3.290774
258.769782	3602.053576	17.018445	-0.050757	3.287365
258.708485	3594.057204	17.023450	-0.050741	3.283934
258.876365	3586.077776	17.028455	-0.050767	3.280515
258.512317	3578.112209	17.033459	-0.050694	3.277078
258.732940	3570.063427	17.038464	-0.050730	3.273624
258.547021	3562.066199	17.043469	-0.050690	3.270173
258.553692	3554.097027	17.048474	-0.050686	3.266738
258.632150	3546.104431	17.053479	-0.050696	3.263292
258.474985	3538.117783	17.058483	-0.050662	3.259835
258.662243	3530.163211	17.063488	-0.050691	3.256403
258.649964	3522.129164	17.068493	-0.050684	3.252924
258.347730	3514.145313	17.073498	-0.050623	3.249452
258.274935	3506.193027	17.078503	-0.050604	3.245999
258.128053	3498.210052	17.083507	-0.050571	3.242526
258.148636	3490.210989	17.088512	-0.050570	3.239049
257.936032	3482.225490	17.093517	-0.050525	3.235565
258.111135	3474.150622	17.098522	-0.050553	3.232054
258.019480	3466.174926	17.103527	-0.050531	3.228571
257.862895	3458.202468	17.108531	-0.050497	3.225084
258.095844	3450.217531	17.113536	-0.050535	3.221603
258.067793	3442.251141	17.118541	-0.050525	3.218115
257.900856	3434.242250	17.123546	-0.050488	3.214600
257.860528	3426.265237	17.128551	-0.050476	3.211100
257.673471	3418.263778	17.133555	-0.050436	3.207579
257.499062	3410.316158	17.138560	-0.050398	3.204079
257.458894	3402.323559	17.143565	-0.050386	3.200560
257.576275	3394.333428	17.148570	-0.050402	3.197046
257.526597	3386.355773	17.153575	-0.050388	3.193526
257.315824	3378.333625	17.158579	-0.050344	3.189975
257.348240	3370.351821	17.163584	-0.050345	3.186449
257.465663	3362.364418	17.168589	-0.050361	3.182920
257.508177	3354.349274	17.173594	-0.050364	3.179371
257.383406	3346.418828	17.178599	-0.050336	3.175849
257.367195	3338.400415	17.183603	-0.050328	3.172289
257.321356	3330.411404	17.188608	-0.050314	3.168737
257.146162	3322.426261	17.193613	-0.050276	3.165176
257.133945	3314.471645	17.198618	-0.050269	3.161632
257.098966	3306.486169	17.203623	-0.050257	3.158070
256.944821	3298.475102	17.208627	-0.050224	3.154487
256.868696	3290.441235	17.213632	-0.050204	3.150893
256.688427	3282.461537	17.218637	-0.050166	3.147314
256.599894	3274.477221	17.223642	-0.050144	3.143734
256.577194	3266.508858	17.228647	-0.050135	3.140159
256.803612	3258.525981	17.233651	-0.050172	3.136585
256.725369	3250.536054	17.238656	-0.050152	3.132990
256.595988	3242.530534	17.243661	-0.050123	3.129381
256.587151	3234.546034	17.248666	-0.050116	3.125783
256.668714	3226.601967	17.253671	-0.050126	3.122204
256.546230	3218.609688	17.258675	-0.050098	3.118589
256.460669	3210.644488	17.263680	-0.050077	3.114984
256.376125	3202.620901	17.268685	-0.050057	3.111349
256.311347	3194.623368	17.273690	-0.050039	3.107721
256.172198	3186.669412	17.278695	-0.050008	3.104106
256.078392	3178.664644	17.283699	-0.049986	3.100466
256.245397	3170.695474	17.288704	-0.050012	3.096850
256.120741	3162.702297	17.293709	-0.049984	3.093205
256.205301	3154.665501	17.298714	-0.049994	3.089545
256.117529	3146.725884	17.303719	-0.049973	3.085918
255.928734	3138.756630	17.308723	-0.049933	3.082268
255.900371	3130.767126	17.313728	-0.049922	3.078612
255.870423	3122.758678	17.318733	-0.049911	3.074942
255.693534	3114.718858	17.323738	-0.049873	3.071247
255.730606	3106.746659	17.328743	-0.049875	3.067589
255.676625	3098.725989	17.333747	-0.049860	3.063900
255.725540	3090.775739	17.338752	-0.049864	3.060243
255.790600	3082.831294	17.343757	-0.049871	3.056586
255.732002	3074.827102	17.348762	-0.049855	3.052891
255.341658	3066.889508	17.353767	-0.049777	3.049206
255.164995	3058.875057	17.358771	-0.049739	3.045491
255.360461	3050.910468	17.363776	-0.049771	3.041813
255.306113	3042.927248	17.368781	-0.049755	3.038110
255.154906	3034.930155	17.373786	-0.049722	3.034391
255.308540	3026.918877	17.378791	-0.049746	3.030675
255.262773	3018.939301	17.383795	-0.049732	3.026960
255.299457	3010.942922	17.388800	-0.049734	3.023237
255.243271	3002.983407	17.393805	-0.049718	3.019522
254.909946	2995.035137	17.398810	-0.049651	3.015794
255.106904	2987.003602	17.403815	-0.049683	3.012048
254.998287	2979.016511	17.408819	-0.049657	3.008304
255.055368	2971.046061	17.413824	-0.049663	3.004570
254.842447	2963.121082	17.418829	-0.049618	3.000841
254.890523	2955.118924	17.423834	-0.049622	2.997083
254.848610	2947.108389	17.428839	-0.049609	2.993312
254.779053	2939.069160	17.433843	-0.049591	2.989521
254.753362	2931.109617	17.438848	-0.049581	2.985765
254.647558	2923.149416	17.443853	-0.049556	2.982000
254.790061	2915.144657	17.448858	-0.049578	2.978222
254.927283	2907.189420	17.453863	-0.049598	2.974462
254.510921	2899.207589	17.458867	-0.049516	2.970657
254.458049	2891.236933	17.463872	-0.049501	2.966871
254.397563	2883.248410	17.468877	-0.049484	2.963071
254.342575	2875.283348	17.473882	-0.049469	2.959277
254.255755	2867.326046	17.478887	-0.049448	2.955481
254.275258	2859.276066	17.483891	-0.049446	2.951641
254.257711	2851.287552	17.488896	-0.049438	2.947823
254.063463	2843.327116	17.493901	-0.049397	2.944005
253.942862	2835.343115	17.498906	-0.049369	2.940174
254.002621	2827.393678	17.503911	-0.049375	2.936364
253.873244	2819.379504	17.508915	-0.049346	2.932509
254.051032	2811.368582	17.513920	-0.049374	2.928665
253.954820	2803.407566	17.518925	-0.049351	2.924827
253.768608	2795.456494	17.523930	-0.049311	2.920983
253.732080	2787.501607	17.528935	-0.049299	2.917141
253.675248	2779.449728	17.533939	-0.049284	2.913245
253.541319	2771.433843	17.538944	-0.049254	2.909358
253.406674	2763.480312	17.543949	-0.049223	2.905495
253.524636	2755.496196	17.548954	-0.049240	2.901626
253.617424	2747.526077	17.553959	-0.049252	2.897757
253.327241	2739.549775	17.558963	-0.049193	2.893860
253.209589	2731.561490	17.563968	-0.049166	2.889960
253.331637	2723.585035	17.568973	-0.049184	2.886074
253.476668	2715.606496	17.573978	-0.049206	2.882184
253.236410	2707.655267	17.578983	-0.049156	2.878280
253.015708	2699.685401	17.583987	-0.049110	2.874363
252.947341	2691.695567	17.588992	-0.049092	2.870439
252.881935	2683.705572	17.593997	-0.049075	2.866509
252.932044	2675.706049	17.599002	-0.049079	2.862576
252.864485	2667.762327	17.604007	-0.049061	2.858659
252.797563	2659.778871	17.609011	-0.049044	2.854716
252.694719	2651.781466	17.614016	-0.049020	2.850759
252.680206	2643.816811	17.619021	-0.049012	2.846818
252.755501	2635.822214	17.624026	-0.049021	2.842862
252.793088	2627.859942	17.629031	-0.049023	2.838913
252.603300	2619.867877	17.634035	-0.048982	2.834932
252.578624	2611.872826	17.639040	-0.048972	2.830953
252.616525	2603.895702	17.644045	-0.048974	2.826981
252.420105	2595.927018	17.649050	-0.048933	2.822994
252.381182	2587.975490	17.654055	-0.048920	2.819019
252.333729	2579.975688	17.659059	-0.048906	2.815014
252.220460	2571.992949	17.664064	-0.048880	2.811008
252.231251	2564.006829	17.669069	-0.048877	2.807002
252.037792	2556.060492	17.674074	-0.048836	2.802998
251.977440	2548.101026	17.679079	-0.048820	2.798989
251.971281	2540.077422	17.684083	-0.048814	2.794945
252.087281	2532.084735	17.689088	-0.048830	2.790919
251.993749	2524.114127	17.694093	-0.048808	2.786885
251.849438	2516.160365	17.699098	-0.048776	2.782851
251.835914	2508.190139	17.704103	-0.048768	2.778811
251.747250	2500.220563	17.709107	-0.048746	2.774760
251.632351	2492.239331	17.714112	-0.048720	2.770696
251.535729	2484.275711	17.719117	-0.048697	2.766636
251.625246	2476.274591	17.724122	-0.048708	2.762562
251.645645	2468.328123	17.729127	-0.048707	2.758506
251.400507	2460.348744	17.734131	-0.048656	2.754411
251.532244	2452.283593	17.739136	-0.048676	2.750289
251.666554	2444.299498	17.744141	-0.048696	2.746202
251.306329	2436.356813	17.749146	-0.048624	2.742101
251.299722	2428.408822	17.754151	-0.048617	2.738012
251.159716	2420.437578	17.759155	-0.048586	2.733897
251.183937	2412.424543	17.764160	-0.048585	2.729764
251.122708	2404.476001	17.769165	-0.048569	2.725653
251.021694	2396.509841	17.774170	-0.048545	2.721524
251.137152	2388.552390	17.779175	-0.048562	2.717407
250.938995	2380.570914	17.784179	-0.048520	2.713252
250.915097	2372.563015	17.789184	-0.048510	2.709087
251.044695	2364.577883	17.794189	-0.048529	2.704937
250.887692	2356.642175	17.799194	-0.048495	2.700789
250.855870	2348.697786	17.804199	-0.048484	2.696638
250.792288	2340.680599	17.809203	-0.048467	2.692440
250.682259	2332.722612	17.814208	-0.048441	2.688263
250.681178	2324.760378	17.819213	-0.048436	2.684085
250.496133	2316.797687	17.824218	-0.048396	2.679889
250.497943	2308.847541	17.829223	-0.048392	2.675704
250.300402	2300.839847	17.834227	-0.048350	2.671470
250.477809	2292.825555	17.839232	-0.048378	2.667249
250.432633	2284.863812	17.844237	-0.048364	2.663035
250.289868	2276.910059	17.849242	-0.048332	2.658813
250.409408	2268.938872	17.854247	-0.048350	2.654591
250.266690	2260.941809	17.859251	-0.048318	2.650332
250.224861	2252.981996	17.864256	-0.048305	2.646093
250.106003	2245.039111	17.869261	-0.048278	2.641850
249.953123	2237.093354	17.874266	-0.048244	2.637597
250.072227	2229.097108	17.879271	-0.048261	2.633328
249.838606	2221.098269	17.884275	-0.048213	2.629028
249.836655	2213.130077	17.889280	-0.048207	2.624752
249.891569	2205.180047	17.894285	-0.048213	2.620482
249.877146	2197.189495	17.899290	-0.048205	2.616180
249.863817	2189.231048	17.904295	-0.048197	2.611887
249.868665	2181.243876	17.909299	-0.048193	2.607573
249.616890	2173.326815	17.914304	-0.048141	2.603273
249.397848	2165.384379	17.919309	-0.048095	2.598954
249.603176	2157.349333	17.924314	-0.048128	2.594606
249.637982	2149.178779	17.929319	-0.048130	2.590166
249.473296	2141.267585	17.934323	-0.048094	2.585846
249.337315	2133.351540	17.939328	-0.048063	2.581517
249.337286	2125.410427	17.944333	-0.048058	2.577178
249.290852	2117.434086	17.949338	-0.048045	2.572808
249.162158	2109.494446	17.954343	-0.048016	2.568445
249.140510	2101.517428	17.959347	-0.048007	2.564062
248.957685	2093.594199	17.964352	-0.047967	2.559690
248.805563	2085.663762	17.969357	-0.047934	2.555308
248.814028	2077.638879	17.974362	-0.047931	2.550878
248.859799	2069.673682	17.979367	-0.047934	2.546475
248.708125	2061.712621	17.984371	-0.047901	2.542054
248.684539	2053.757953	17.989376	-0.047891	2.537637
248.628321	2045.792398	17.994381	-0.047876	2.533204
248.659840	2037.797444	17.999386	-0.047876	2.528753
248.606690	2029.853889	18.004391	-0.047861	2.524318
248.429465	2021.902497	18.009395	-0.047823	2.519861
248.405671	2013.969610	18.014400	-0.047814	2.515417
248.224655	2005.956331	18.019405	-0.047775	2.510909
248.348203	1997.940408	18.024410	-0.047793	2.506414
248.402963	1990.004414	18.029415	-0.047798	2.501950
248.273772	1982.049517	18.034419	-0.047769	2.497455
248.292141	1974.084206	18.039424	-0.047767	2.492956
248.138646	1966.119336	18.044429	-0.047734	2.488437
248.018530	1958.169112	18.049434	-0.047706	2.483920
248.100535	1950.218511	18.054439	-0.047716	2.479409
247.955195	1942.259173	18.059443	-0.047684	2.474869
247.893969	1934.265037	18.064448	-0.047668	2.470307
247.875323	1926.298730	18.069453	-0.047659	2.465755
247.925550	1918.332992	18.074458	-0.047663	2.461200
248.007970	1910.390819	18.079463	-0.047674	2.456653
247.849590	1902.407311	18.084467	-0.047639	2.452056
247.699546	1894.459730	18.089472	-0.047606	2.447471
247.794700	1886.517192	18.094477	-0.047619	2.442899
247.604800	1878.564480	18.099482	-0.047578	2.438291
247.469510	1870.600609	18.104487	-0.047548	2.433672
247.271572	1862.579221	18.109491	-0.047506	2.429005
247.401389	1854.606148	18.114496	-0.047525	2.424383
247.381935	1846.668422	18.119501	-0.047516	2.419762
247.265515	1838.717497	18.124506	-0.047490	2.415116
247.384096	1830.743629	18.129511	-0.047507	2.410466
247.099951	1822.800878	18.134515	-0.047449	2.405794
247.048610	1814.864366	18.139520	-0.047434	2.401135
247.028377	1806.924818	18.144525	-0.047425	2.396467
247.035864	1798.917075	18.149530	-0.047422	2.391752
246.907707	1790.980986	18.154535	-0.047393	2.387060
246.837240	1783.014889	18.159539	-0.047374	2.382345
246.650097	1775.097838	18.164544	-0.047334	2.377640
246.657962	1767.131835	18.169549	-0.047331	2.372913
246.655493	1759.131947	18.174554	-0.047325	2.368155
246.858989	1751.171237	18.179559	-0.047358	2.363427
246.418248	1743.283436	18.184563	-0.047271	2.358682
246.289478	1735.328074	18.189568	-0.047242	2.353912
246.285696	1727.328879	18.194573	-0.047236	2.349116
246.220177	1719.348641	18.199578	-0.047219	2.344316
246.181901	1711.429274	18.204583	-0.047207	2.339545
246.247331	1703.453864	18.209587	-0.047214	2.334740
246.196910	1695.478804	18.214592	-0.047199	2.329915
246.047406	1687.549192	18.219597	-0.047166	2.325099
245.892766	1679.619582	18.224602	-0.047133	2.320273
245.969415	1671.672235	18.229607	-0.047142	2.315446
245.895675	1663.683121	18.234611	-0.047123	2.310570
245.845804	1655.730878	18.239616	-0.047109	2.305708
246.078381	1647.762138	18.244621	-0.047147	2.300850
245.850134	1639.844975	18.249626	-0.047099	2.295974
245.560090	1631.918498	18.254631	-0.047040	2.291077
245.611674	1623.924250	18.259635	-0.047045	2.286157
245.749296	1615.974224	18.264640	-0.047065	2.281260
245.530757	1608.075107	18.269645	-0.047019	2.276355
245.417022	1600.045661	18.274650	-0.046993	2.271366
245.517923	1592.063232	18.279655	-0.047007	2.266415
245.467335	1584.128389	18.284659	-0.046992	2.261469
245.318609	1576.208533	18.289664	-0.046960	2.256513
245.382673	1568.248972	18.294669	-0.046966	2.251540
245.305705	1560.291462	18.299674	-0.046947	2.246545
245.249371	1552.374133	18.304679	-0.046932	2.241565
245.110222	1544.442378	18.309683	-0.046901	2.236558
245.052910	1536.482707	18.314688	-0.046885	2.231530
245.215138	1528.500963	18.319693	-0.046910	2.226496
244.690397	1520.623169	18.324698	-0.046807	2.221455
244.924049	1512.654416	18.329703	-0.046846	2.216412
244.839451	1504.691222	18.334707	-0.046825	2.211333
244.579055	1496.767156	18.339712	-0.046771	2.206252
244.471041	1488.847390	18.344717	-0.046746	2.201175
244.520432	1480.888284	18.349722	-0.046750	2.196075
244.629348	1472.898951	18.354727	-0.046765	2.190950
244.422736	1464.967951	18.359731	-0.046722	2.185821
244.484297	1457.027419	18.364736	-0.046728	2.180698
244.305737	1449.113243	18.369741	-0.046690	2.175559
244.205813	1441.142330	18.374746	-0.046666	2.170378
244.255544	1433.198494	18.379751	-0.046670	2.165216
243.991029	1425.298873	18.384755	-0.046616	2.160041
243.839211	1417.371533	18.389760	-0.046583	2.154846
243.910463	1409.386848	18.394765	-0.046591	2.149621
243.975405	1401.415994	18.399770	-0.046598	2.144393
244.037254	1393.505454	18.404775	-0.046604	2.139191
243.938117	1385.564380	18.409779	-0.046581	2.133941
243.910229	1377.618546	18.414784	-0.046571	2.128682
243.908036	1369.696889	18.419789	-0.046565	2.123428
243.689249	1361.793835	18.424794	-0.046519	2.118152
243.645330	1353.825087	18.429799	-0.046506	2.112837
243.570724	1345.836267	18.434803	-0.046487	2.107492
243.376325	1337.926467	18.439808	-0.046446	2.102174
243.319159	1330.022077	18.444813	-0.046430	2.096860
243.232686	1322.063032	18.449818	-0.046409	2.091493
243.246123	1314.129612	18.454823	-0.046406	2.086138
243.321041	1306.190097	18.459827	-0.046415	2.080773
243.101444	1298.293796	18.464832	-0.046369	2.075393
243.204661	1290.330806	18.469837	-0.046384	2.069986
242.951051	1282.406687	18.474842	-0.046331	2.064556
243.191114	1274.462561	18.479847	-0.046371	2.059147
243.111096	1266.545622	18.484851	-0.046351	2.053711
242.840146	1258.628185	18.489856	-0.046295	2.048240
242.862851	1250.711232	18.494861	-0.046295	2.042785
242.731549	1242.798055	18.499866	-0.046265	2.037302
242.698720	1234.864355	18.504871	-0.046254	2.031800
242.527825	1226.908521	18.509875	-0.046217	2.026254
242.433857	1218.994792	18.514880	-0.046195	2.020729
242.505444	1211.071650	18.519885	-0.046203	2.015200
242.420293	1203.116559	18.524890	-0.046182	2.009617
242.443237	1195.191373	18.529895	-0.046181	2.004051
242.444213	1187.277475	18.534899	-0.046176	1.998475
242.372220	1179.358065	18.539904	-0.046158	1.992872
242.294726	1171.438236	18.544909	-0.046138	1.987252
241.907194	1163.557964	18.549914	-0.046061	1.981611
242.019507	1155.623411	18.554919	-0.046077	1.975969
241.862005	1147.688351	18.559923	-0.046043	1.970281
241.986993	1139.747643	18.564928	-0.046061	1.964603
241.963172	1131.860012	18.569933	-0.046051	1.958931
241.670975	1123.950169	18.574938	-0.045992	1.953197
241.521355	1116.001019	18.579943	-0.045959	1.947434
241.656459	1108.051712	18.584947	-0.045979	1.941684
241.587816	1100.148259	18.589952	-0.045961	1.935928
241.427902	1092.243600	18.594957	-0.045926	1.930144
241.492328	1084.308088	18.599962	-0.045933	1.924345
241.416410	1076.432008	18.604967	-0.045914	1.918556
241.308108	1068.512205	18.609971	-0.045889	1.912714
241.174033	1060.590366	18.614976	-0.045859	1.906850
241.255543	1052.676349	18.619981	-0.045869	1.900997
241.308721	1044.750615	18.624986	-0.045874	1.895115
241.061564	1036.876775	18.629991	-0.045823	1.889218
240.837940	1028.993263	18.634995	-0.045776	1.883299
240.868931	1021.081840	18.640000	-0.045777	1.877370
240.785932	1013.162990	18.645005	-0.045756	1.871402
240.722986	1005.226317	18.650010	-0.045740	1.865405
240.766697	997.333276	18.655015	-0.045743	1.859433
240.628825	989.433362	18.660019	-0.045712	1.853416
240.624216	981.505867	18.665024	-0.045706	1.847374
240.605217	973.625432	18.670029	-0.045697	1.841346
240.309682	965.763436	18.675034	-0.045637	1.835281
240.234633	957.848631	18.680039	-0.045618	1.829180
240.313125	949.928771	18.685043	-0.045628	1.823073
240.184373	942.050559	18.690048	-0.045599	1.816953
240.135251	934.145995	18.695053	-0.045585	1.810802
239.953541	926.263595	18.700058	-0.045546	1.804631
240.092559	918.371241	18.705063	-0.045567	1.798470
240.011395	910.444814	18.710067	-0.045547	1.792233
239.777815	902.539181	18.715072	-0.045498	1.785973
239.925523	894.641673	18.720077	-0.045520	1.779745
239.843970	886.758760	18.725082	-0.045500	1.773477
239.947839	878.841451	18.730087	-0.045515	1.767183
239.798318	870.983870	18.735091	-0.045482	1.760883
239.569019	863.142473	18.740096	-0.045434	1.754563
239.674461	855.217443	18.745101	-0.045449	1.748194
239.768635	847.300536	18.750106	-0.045461	1.741808
239.649254	839.462082	18.755111	-0.045434	1.735435
239.290446	831.616322	18.760115	-0.045362	1.729001
239.213904	823.738994	18.765120	-0.045343	1.722554
239.245503	815.870771	18.770125	-0.045344	1.716104
239.087058	807.973186	18.775130	-0.045309	1.709581
238.930490	800.107810	18.780135	-0.045275	1.703060
239.016591	792.207171	18.785139	-0.045286	1.696516
239.095654	784.303753	18.790144	-0.045296	1.689944
238.938488	776.474614	18.795149	-0.045261	1.683377
238.659012	768.635347	18.800154	-0.045204	1.676759
238.903779	760.717022	18.805159	-0.045245	1.670118
238.761240	752.863145	18.810163	-0.045213	1.663454
238.549680	745.028499	18.815168	-0.045169	1.656769
238.482312	737.157405	18.820173	-0.045151	1.650046
238.436394	729.288245	18.825178	-0.045138	1.643300
238.304166	721.459883	18.830183	-0.045108	1.636550
238.447857	713.512535	18.835187	-0.045130	1.629706
238.267474	705.670064	18.840192	-0.045091	1.622880
238.285986	697.820845	18.845197	-0.045090	1.616047
238.166501	689.959512	18.850202	-0.045062	1.609155
238.095695	682.127657	18.855207	-0.045044	1.602266
237.998775	674.294129	18.860211	-0.045021	1.595342
237.761585	666.454247	18.865216	-0.044972	1.588362
237.850282	658.597619	18.870221	-0.044983	1.581383
237.732216	650.765074	18.875226	-0.044957	1.574365
237.771557	642.900659	18.880231	-0.044959	1.567310
237.666784	635.080300	18.885235	-0.044934	1.560241
237.827330	627.219858	18.890240	-0.044959	1.553143
237.642587	619.395542	18.895245	-0.044920	1.545994
237.449853	611.586354	18.900250	-0.044879	1.538825
237.437595	603.755932	18.905255	-0.044872	1.531629
237.347403	595.923773	18.910259	-0.044850	1.524386
237.224103	588.119461	18.915264	-0.044822	1.517130
237.239566	580.280652	18.920269	-0.044820	1.509827
237.117137	572.459899	18.925274	-0.044792	1.502485
237.021055	564.663858	18.930279	-0.044769	1.495134
236.959182	556.832090	18.935283	-0.044753	1.487718
237.007085	549.006155	18.940288	-0.044757	1.480287
236.905851	541.207595	18.945293	-0.044733	1.472822
236.407717	533.422534	18.950298	-0.044635	1.465269
236.576908	525.592448	18.955303	-0.044662	1.457739
236.391680	517.801852	18.960307	-0.044622	1.450152
236.235102	510.014227	18.965312	-0.044588	1.442532
236.228276	502.226173	18.970317	-0.044582	1.434896
236.341204	494.377906	18.975322	-0.044598	1.427179
236.244316	486.609926	18.980327	-0.044575	1.419465
236.165886	478.830506	18.985331	-0.044555	1.411701
236.057206	471.048375	18.990336	-0.044530	1.403886
236.253360	463.254148	18.995341	-0.044562	1.396066
235.842143	455.509162	19.000346	-0.044480	1.388150
235.713891	447.750176	19.005351	-0.044451	1.380222
235.684553	439.979121	19.010355	-0.044441	1.372252
235.517483	432.217761	19.015360	-0.044405	1.364222
235.506592	424.468359	19.020365	-0.044398	1.356184
235.368520	416.700503	19.025370	-0.044367	1.348057
235.293690	408.947921	19.030375	-0.044348	1.339908
235.245102	401.197913	19.035379	-0.044334	1.331715
235.150576	393.451204	19.040384	-0.044312	1.323468
235.338290	385.680727	19.045389	-0.044342	1.315194
235.064302	377.845205	19.050394	-0.044286	1.306714
234.927907	370.152037	19.055399	-0.044255	1.298358
234.882805	362.423915	19.060403	-0.044242	1.289926
234.544443	354.754526	19.065408	-0.044174	1.281450
234.428652	347.065674	19.070413	-0.044148	1.272936
234.518347	339.305581	19.075418	-0.044159	1.264325
234.372172	331.629882	19.080423	-0.044127	1.255704
234.288117	323.923009	19.085427	-0.044107	1.247001
234.130149	316.255875	19.090432	-0.044072	1.238267
234.078061	308.554941	19.095437	-0.044058	1.229453
234.029567	300.852850	19.100442	-0.044044	1.220575
233.911118	293.189719	19.105447	-0.044017	1.211663
233.786999	285.522353	19.110451	-0.043989	1.202679
233.664056	277.870520	19.115456	-0.043961	1.193646
233.750752	270.189089	19.120461	-0.043972	1.184551
233.620834	262.546706	19.125466	-0.043943	1.175388
233.512244	254.903537	19.130471	-0.043918	1.166157
233.486454	247.279085	19.135475	-0.043909	1.156892
233.057073	239.663933	19.140480	-0.043824	1.147479
233.124607	232.015490	19.145485	-0.043831	1.138052
232.922333	224.409426	19.150490	-0.043789	1.128541
232.978519	216.791864	19.155495	-0.043795	1.118991
232.601045	209.241848	19.160499	-0.043719	1.109350
232.726398	201.608325	19.165504	-0.043738	1.099627
232.590566	194.046473	19.170509	-0.043708	1.089853
232.466245	186.481641	19.175514	-0.043680	1.079989
232.355655	178.923491	19.180519	-0.043654	1.070046
232.207565	171.375445	19.185523	-0.043622	1.060015
231.917197	163.863694	19.190528	-0.043563	1.049903
231.901567	156.330483	19.195533	-0.043555	1.039728
231.522764	148.853091	19.200538	-0.043480	1.029442
231.382419	141.352845	19.205543	-0.043449	1.019079
231.204725	133.864912	19.210547	-0.043411	1.008617
230.839068	126.426638	19.215552	-0.043339	0.998069
230.458724	118.970226	19.220557	-0.043263	0.987379
229.967428	111.559352	19.225562	-0.043167	0.976609
229.478428	104.166149	19.230567	-0.043071	0.965745
229.149229	96.760421	19.235571	-0.043005	0.954781
228.759299	89.363202	19.240576	-0.042928	0.943685
228.404310	81.990892	19.245581	-0.042857	0.932504
227.908092	74.646342	19.250586	-0.042760	0.921192
227.400424	67.324776	19.255591	-0.042661	0.909772
226.898217	60.239319	19.260595	-0.042563	0.898578