Tue Mar 23 11:36:52 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.627688	-0.054724	0.000000	-0.000009	0.722771

0.457249	-0.063808	0.005005	0.000022	0.722694
0.543739	-0.076963	0.010010	0.000006	0.722699
0.487090	-0.065790	0.015014	0.000017	0.722701
0.555022	-0.082082	0.020019	0.000004	0.722693
0.720600	-0.106016	0.025024	-0.000027	0.722704
0.613498	-0.090672	0.030029	-0.000007	0.722697
0.525682	-0.075262	0.035034	0.000009	0.722697
0.615371	-0.089504	0.040038	-0.000008	0.722700
0.679983	-0.105086	0.045043	-0.000020	0.722692
0.585546	-0.084283	0.050048	-0.000002	0.722701
0.702826	-0.107214	0.055053	-0.000024	0.722697
0.590035	-0.086881	0.060058	-0.000004	0.722697
0.449710	-0.060812	0.065062	0.000022	0.722700
0.484360	-0.070424	0.070067	0.000016	0.722693
0.782061	-0.160734	0.075072	-0.000040	0.722620
0.708529	-0.275172	0.080077	-0.000026	0.722370
0.597128	-0.252424	0.085082	-0.000005	0.722376
0.581755	-0.248877	0.090086	-0.000003	0.722378
0.458753	-0.231972	0.095091	0.000020	0.722368
0.513960	-0.237414	0.100096	0.000010	0.722377
0.515057	-0.240614	0.105101	0.000010	0.722371
0.602406	-0.371095	0.110106	-0.000007	0.722146
0.680175	-0.418094	0.115110	-0.000021	0.722081
0.474703	-0.384241	0.120115	0.000017	0.722075
0.651659	-0.412630	0.125120	-0.000016	0.722082
0.593657	-0.406698	0.130125	-0.000006	0.722073
0.550900	-0.534856	0.135130	0.000002	0.721807
0.600407	-0.572402	0.140134	-0.000007	0.721750
0.543026	-0.565387	0.145139	0.000004	0.721744
0.545890	-0.562547	0.150144	0.000003	0.721751
0.488915	-0.646158	0.155149	0.000014	0.721567
0.527681	-0.716431	0.160154	0.000006	0.721443
0.486476	-0.707850	0.165158	0.000014	0.721445
0.566474	-0.726482	0.170163	-0.000001	0.721437
0.597292	-0.864128	0.175168	-0.000007	0.721177
0.221767	-0.825700	0.180173	0.000063	0.721121
0.417929	-0.859459	0.185178	0.000026	0.721124
0.422901	-0.909873	0.190182	0.000025	0.721027
0.293387	-0.962908	0.195187	0.000049	0.720877
0.302746	-0.960197	0.200192	0.000047	0.720886
0.402035	-1.011249	0.205197	0.000029	0.720820
0.336522	-1.139796	0.210202	0.000041	0.720545
0.373370	-1.145787	0.215206	0.000034	0.720546
0.301132	-1.172586	0.220211	0.000047	0.720468
0.305691	-1.293809	0.225216	0.000047	0.720231
0.516015	-1.335521	0.230221	0.000007	0.720223
0.446762	-1.402923	0.235226	0.000020	0.720066
0.551012	-1.501675	0.240230	0.000001	0.719908
0.437146	-1.486693	0.245235	0.000022	0.719898
0.425067	-1.618517	0.250240	0.000024	0.719634
0.285574	-1.608589	0.255245	0.000050	0.719605
0.305298	-1.688480	0.260250	0.000046	0.719454
0.047414	-1.733603	0.265254	0.000094	0.719275
-0.285305	-1.677074	0.270259	0.000156	0.719270
-0.195641	-1.837338	0.275264	0.000139	0.718985
0.018675	-1.887469	0.280269	0.000099	0.718962
-0.251208	-1.920586	0.285274	0.000149	0.718802
-0.120603	-2.021795	0.290278	0.000125	0.718648
-0.213828	-2.036805	0.295283	0.000142	0.718586
-0.166565	-2.160062	0.300288	0.000133	0.718360
-0.324854	-2.134785	0.305293	0.000163	0.718354
-0.481796	-2.264855	0.310298	0.000192	0.718042
-2.755182	-1.868615	0.315302	0.000615	0.718025
-2.144661	-2.018276	0.320307	0.000501	0.717945
-2.727688	-2.033012	0.325312	0.000610	0.717710
-3.372077	-1.921442	0.330317	0.000730	0.717704
-3.285031	-1.936613	0.335322	0.000713	0.717705
-3.248404	-2.090030	0.340326	0.000706	0.717415
-4.515731	-1.882081	0.345331	0.000942	0.717380
-4.327177	-1.911620	0.350336	0.000907	0.717388
-3.793808	-2.047036	0.355341	0.000808	0.717309
-5.287814	-1.893940	0.360346	0.001086	0.717085
-4.814337	-1.976117	0.365350	0.000997	0.717090
-4.898861	-1.965625	0.370355	0.001013	0.717081
-4.875040	-2.002431	0.375360	0.001008	0.717017
-5.732364	-1.982421	0.380365	0.001168	0.716754
-5.733886	-1.981031	0.385370	0.001168	0.716757
-5.880945	-1.952265	0.390374	0.001195	0.716762
-6.236853	-1.892492	0.395379	0.001262	0.716755
-5.981462	-2.027639	0.400384	0.001214	0.716578
-6.694532	-1.964434	0.405389	0.001347	0.716452
-6.781529	-1.950896	0.410394	0.001363	0.716448
-6.810427	-1.941677	0.415398	0.001368	0.716456
-6.951151	-1.922550	0.420403	0.001394	0.716445
-6.482060	-2.114784	0.425408	0.001307	0.716229
-7.904198	-1.909229	0.430413	0.001571	0.716135
-7.975989	-1.897925	0.435418	0.001584	0.716132
-7.291296	-2.017138	0.440422	0.001457	0.716138
-7.800643	-1.930859	0.445427	0.001552	0.716129
-7.870097	-1.959436	0.450432	0.001564	0.716048
-8.347540	-1.957672	0.455437	0.001653	0.715884
-8.593420	-1.914456	0.460442	0.001699	0.715883
-8.602456	-1.908935	0.465446	0.001700	0.715891
-8.671677	-1.902341	0.470451	0.001713	0.715879
-8.362513	-1.951484	0.475456	0.001656	0.715891
-8.707817	-1.973471	0.480461	0.001720	0.715726
-9.950490	-1.841709	0.485466	0.001951	0.715549
-8.931097	-2.020659	0.490470	0.001761	0.715554
-9.540272	-1.917617	0.495475	0.001874	0.715543
-9.765016	-1.871828	0.500480	0.001916	0.715555
-9.240514	-1.968184	0.505485	0.001818	0.715549
-9.402345	-1.990818	0.510490	0.001848	0.715448
-10.459132	-1.906363	0.515494	0.002045	0.715242
-10.362022	-1.929074	0.520499	0.002027	0.715231
-10.361879	-1.924522	0.525504	0.002027	0.715241
-10.283754	-1.942160	0.530509	0.002012	0.715234
-10.457650	-1.911331	0.535514	0.002044	0.715233
-10.322363	-1.933800	0.540518	0.002019	0.715237
-10.927780	-1.968791	0.545523	0.002132	0.714954
-11.397407	-1.904906	0.550528	0.002219	0.714915
-11.415988	-1.903666	0.555533	0.002222	0.714911
-11.207031	-1.942129	0.560538	0.002183	0.714908
-11.248112	-1.930867	0.565542	0.002191	0.714917
-11.563685	-1.879244	0.570547	0.002250	0.714908
-10.975688	-1.987933	0.575552	0.002140	0.714900
-11.839968	-1.980555	0.580557	0.002301	0.714609
-12.417751	-1.876841	0.585562	0.002408	0.714611
-11.866436	-1.973573	0.590566	0.002306	0.714614
-11.907115	-1.968514	0.595571	0.002313	0.714610
-12.355011	-1.885931	0.600576	0.002396	0.714616
-12.513525	-1.858744	0.605581	0.002426	0.714614
-12.282336	-1.921405	0.610586	0.002383	0.714571
-12.924536	-1.950957	0.615590	0.002502	0.714286
-13.363399	-1.877681	0.620595	0.002584	0.714276
-13.210341	-1.901906	0.625600	0.002555	0.714282
-12.891852	-1.960076	0.630605	0.002496	0.714280
-13.119770	-1.920486	0.635610	0.002538	0.714278
-12.984615	-1.942700	0.640614	0.002513	0.714282
-13.167947	-1.925389	0.645619	0.002547	0.714252
-13.802241	-1.952234	0.650624	0.002665	0.713974
-13.814717	-1.951844	0.655629	0.002667	0.713970
-14.110448	-1.899623	0.660634	0.002722	0.713970
-14.146078	-1.889768	0.665638	0.002728	0.713977
-14.387195	-1.853283	0.670643	0.002773	0.713964
-14.120828	-1.896516	0.675648	0.002723	0.713973
-13.930550	-1.930514	0.680653	0.002688	0.713973
-14.705455	-1.925934	0.685658	0.002832	0.713708
-15.129449	-1.875746	0.690662	0.002911	0.713657
-15.129505	-1.880589	0.695667	0.002911	0.713648
-15.057449	-1.889722	0.700672	0.002897	0.713656
-15.336287	-1.842667	0.705677	0.002949	0.713651
-15.394265	-1.833307	0.710682	0.002960	0.713649
-14.914337	-1.914389	0.715686	0.002870	0.713658
-15.117043	-1.887881	0.720691	0.002908	0.713639
-15.392688	-1.977268	0.725696	0.002959	0.713364
-15.662654	-1.931360	0.730701	0.003009	0.713360
-16.134963	-1.848780	0.735706	0.003097	0.713357
-15.325685	-1.989908	0.740710	0.002946	0.713363
-15.680735	-1.932099	0.745715	0.003012	0.713352
-16.076776	-1.858595	0.750720	0.003086	0.713358
-15.811354	-1.964502	0.755725	0.003036	0.713242
-17.043158	-1.858973	0.760730	0.003266	0.713015
-16.823031	-1.894644	0.765734	0.003225	0.713023
-17.057242	-1.856320	0.770739	0.003268	0.713016
-16.797861	-1.900042	0.775744	0.003220	0.713021
-16.507167	-1.952127	0.780749	0.003166	0.713021
-16.898955	-1.882712	0.785754	0.003238	0.713020
-16.852071	-1.888580	0.790758	0.003229	0.713026
-17.389781	-1.944362	0.795763	0.003330	0.712724
-17.814129	-1.873535	0.800768	0.003408	0.712715
-17.851962	-1.867447	0.805773	0.003415	0.712714
-17.694922	-1.896154	0.810778	0.003386	0.712712
-17.712759	-1.891121	0.815782	0.003389	0.712716
-17.958343	-1.852884	0.820787	0.003435	0.712705
-17.612835	-1.911599	0.825792	0.003370	0.712711
-17.897376	-1.951061	0.830797	0.003423	0.712532
-19.191629	-1.794560	0.835802	0.003664	0.712385
-18.577933	-1.900624	0.840806	0.003550	0.712391
-18.485747	-1.920950	0.845811	0.003532	0.712384
-18.856120	-1.851900	0.850816	0.003601	0.712390
-18.701923	-1.880336	0.855821	0.003572	0.712388
-18.837951	-1.859223	0.860826	0.003598	0.712382
-18.753966	-1.877344	0.865830	0.003582	0.712376
-19.704727	-1.854262	0.870835	0.003759	0.712085
-19.522764	-1.882437	0.875840	0.003725	0.712094
-19.538872	-1.881277	0.880845	0.003728	0.712090
-19.396434	-1.907265	0.885850	0.003701	0.712089
-19.541378	-1.878885	0.890854	0.003728	0.712095
-19.645493	-1.863651	0.895859	0.003747	0.712088
-19.478468	-1.891240	0.900864	0.003716	0.712093
-19.691407	-1.979893	0.905869	0.003756	0.711841
-20.645296	-1.850015	0.910874	0.003933	0.711761
-20.278456	-1.912422	0.915878	0.003865	0.711767
-20.538918	-1.868354	0.920883	0.003913	0.711763
-20.713736	-1.836295	0.925888	0.003946	0.711765
-20.293666	-1.911277	0.930893	0.003867	0.711764
-20.705483	-1.839970	0.935898	0.003944	0.711761
-20.795702	-1.912786	0.940902	0.003961	0.711583
-21.511879	-1.850551	0.945907	0.004094	0.711453
-21.235330	-1.898516	0.950912	0.004042	0.711456
-21.483204	-1.855398	0.955917	0.004088	0.711454
-21.643357	-1.828769	0.960922	0.004118	0.711451
-21.376348	-1.871906	0.965926	0.004068	0.711460
-21.572232	-1.841883	0.970931	0.004104	0.711450
-21.536581	-1.870596	0.975936	0.004098	0.711406
-21.772492	-1.961320	0.980941	0.004142	0.711141
-22.077157	-1.910038	0.985946	0.004198	0.711135
-22.442254	-1.840129	0.990950	0.004266	0.711145
-22.288944	-1.872591	0.995955	0.004237	0.711135
-22.293864	-1.868925	1.000960	0.004238	0.711141
-22.716257	-1.793344	1.005965	0.004317	0.711142
-22.310378	-1.869906	1.010970	0.004241	0.711133
-22.541519	-1.957283	1.015974	0.004284	0.710877
-23.379922	-1.812662	1.020979	0.004440	0.710868
-23.409515	-1.803859	1.025984	0.004445	0.710875
-22.714162	-1.928830	1.030989	0.004316	0.710873
-23.260876	-1.834654	1.035994	0.004417	0.710867
-23.250124	-1.831358	1.040998	0.004415	0.710877
-23.138897	-1.854836	1.046003	0.004395	0.710870
-23.629097	-1.934838	1.051008	0.004486	0.710536
-24.343570	-1.808425	1.056013	0.004619	0.710535
-24.524000	-1.778296	1.061018	0.004652	0.710531
-23.785429	-1.905226	1.066022	0.004514	0.710540
-24.119961	-1.850687	1.071027	0.004577	0.710530
-24.313770	-1.813721	1.076032	0.004613	0.710535
-24.077615	-1.855120	1.081037	0.004569	0.710537
-24.527155	-1.870705	1.086042	0.004652	0.710346
-25.357509	-1.784598	1.091046	0.004807	0.710223
-24.726602	-1.900668	1.096051	0.004689	0.710216
-24.655321	-1.910935	1.101056	0.004676	0.710221
-25.314814	-1.792948	1.106061	0.004798	0.710222
-25.155159	-1.824934	1.111066	0.004768	0.710215
-24.640179	-1.911953	1.116070	0.004673	0.710225
-25.152167	-1.895443	1.121075	0.004768	0.710075
-26.210336	-1.797091	1.126080	0.004965	0.709895
-25.465571	-1.930053	1.131085	0.004826	0.709895
-25.870696	-1.861055	1.136090	0.004901	0.709889
-25.822357	-1.864075	1.141094	0.004892	0.709900
-25.546139	-1.918469	1.146099	0.004841	0.709890
-25.681997	-1.889956	1.151104	0.004866	0.709899
-26.155751	-1.902733	1.156109	0.004954	0.709705
-27.015355	-1.804679	1.161114	0.005114	0.709595
-26.638925	-1.867370	1.166118	0.005044	0.709604
-26.763479	-1.850859	1.171123	0.005067	0.709592
-27.015272	-1.802197	1.176128	0.005113	0.709600
-26.784647	-1.844136	1.181133	0.005070	0.709599
-26.878163	-1.831283	1.186138	0.005088	0.709591
-26.760812	-1.890369	1.191142	0.005066	0.709515
-27.712841	-1.847110	1.196147	0.005243	0.709262
-27.167383	-1.941952	1.201152	0.005141	0.709267
-27.649009	-1.856431	1.206157	0.005231	0.709267
-27.814751	-1.828367	1.211162	0.005262	0.709264
-27.429393	-1.893316	1.216166	0.005190	0.709272
-27.794261	-1.830784	1.221171	0.005258	0.709267
-27.579007	-1.928076	1.226176	0.005217	0.709149
-28.286165	-1.895955	1.231181	0.005349	0.708962
-28.271608	-1.902161	1.236186	0.005346	0.708955
-28.380394	-1.879763	1.241190	0.005366	0.708961
-28.722032	-1.822614	1.246195	0.005430	0.708954
-28.508767	-1.858031	1.251200	0.005390	0.708959
-28.413397	-1.873570	1.256205	0.005372	0.708962
-28.649321	-1.907508	1.261210	0.005416	0.708810
-29.398765	-1.856038	1.266214	0.005555	0.708646
-29.104153	-1.914055	1.271219	0.005500	0.708635
-29.608464	-1.820008	1.276224	0.005594	0.708644
-29.440905	-1.848763	1.281229	0.005563	0.708646
-29.375263	-1.865667	1.286234	0.005550	0.708636
-29.368210	-1.862003	1.291238	0.005549	0.708646
-29.656796	-1.851622	1.296243	0.005603	0.708564
-30.142658	-1.870647	1.301248	0.005693	0.708352
-29.950842	-1.904971	1.306253	0.005657	0.708352
-30.767850	-1.762445	1.311258	0.005809	0.708346
-30.398248	-1.823467	1.316262	0.005740	0.708356
-30.122550	-1.876983	1.321267	0.005689	0.708348
-30.576405	-1.795627	1.326272	0.005773	0.708349
-30.443004	-1.818218	1.331277	0.005748	0.708351
-30.547661	-1.965976	1.336282	0.005768	0.708018
-31.031848	-1.881665	1.341286	0.005858	0.708014
-31.625181	-1.779148	1.346291	0.005968	0.708008
-31.130630	-1.865204	1.351296	0.005876	0.708012
-30.946376	-1.897675	1.356301	0.005842	0.708013
-31.522706	-1.799201	1.361306	0.005949	0.708005
-31.327161	-1.828586	1.366310	0.005912	0.708016
-31.680276	-1.899891	1.371315	0.005978	0.707747
-32.447936	-1.785328	1.376320	0.006121	0.707703
-32.206385	-1.828634	1.381325	0.006076	0.707702
-32.054469	-1.860284	1.386330	0.006047	0.707694
-32.236645	-1.823372	1.391334	0.006081	0.707703
-32.300512	-1.816763	1.396339	0.006093	0.707693
-31.985731	-1.870784	1.401344	0.006034	0.707698
-32.113085	-1.924508	1.406349	0.006058	0.707545
-33.378579	-1.784523	1.411354	0.006293	0.707373
-32.787364	-1.885244	1.416358	0.006183	0.707383
-32.951564	-1.859741	1.421363	0.006213	0.707375
-33.057000	-1.839383	1.426368	0.006233	0.707379
-32.877292	-1.870697	1.431373	0.006199	0.707380
-33.196108	-1.817367	1.436378	0.006259	0.707373
-33.110972	-1.888318	1.441382	0.006243	0.707262
-33.935861	-1.831867	1.446387	0.006396	0.707080
-33.721333	-1.868765	1.451392	0.006356	0.707083
-33.738701	-1.864880	1.456397	0.006359	0.707085
-34.103399	-1.804148	1.461402	0.006427	0.707076
-33.564775	-1.895113	1.466406	0.006327	0.707087
-33.810257	-1.854383	1.471411	0.006372	0.707081
-34.234353	-1.867702	1.476416	0.006451	0.706902
-35.060180	-1.794056	1.481421	0.006605	0.706755
-34.652728	-1.870039	1.486426	0.006529	0.706748
-34.573049	-1.879876	1.491430	0.006514	0.706757
-34.981888	-1.809953	1.496435	0.006590	0.706752
-34.686897	-1.861931	1.501440	0.006535	0.706753
-34.474802	-1.897037	1.506445	0.006495	0.706759
-34.928941	-1.875674	1.511450	0.006580	0.706639
-35.709662	-1.828946	1.516454	0.006725	0.706454
-35.472709	-1.876018	1.521459	0.006681	0.706444
-35.900095	-1.798826	1.526464	0.006760	0.706446
-35.823380	-1.811243	1.531469	0.006746	0.706449
-35.799875	-1.818759	1.536474	0.006741	0.706443
-35.520629	-1.863467	1.541478	0.006689	0.706453
-35.747528	-1.844799	1.546483	0.006731	0.706410
-36.512648	-1.846655	1.551488	0.006874	0.706132
-36.301806	-1.883871	1.556493	0.006834	0.706133
-36.922325	-1.777224	1.561498	0.006950	0.706125
-36.564090	-1.836130	1.566502	0.006883	0.706135
-36.189112	-1.906326	1.571507	0.006813	0.706129
-36.588301	-1.833925	1.576512	0.006887	0.706131
-36.578748	-1.847763	1.581517	0.006885	0.706107
-37.146490	-1.868168	1.586522	0.006991	0.705863
-37.039040	-1.884746	1.591526	0.006971	0.705868
-37.610066	-1.786839	1.596531	0.007077	0.705861
-37.381164	-1.825762	1.601536	0.007034	0.705865
-36.887742	-1.912063	1.606541	0.006942	0.705868
-37.405351	-1.822979	1.611546	0.007039	0.705862
-37.215951	-1.937369	1.616550	0.007003	0.705700
-38.301096	-1.832018	1.621555	0.007205	0.705523
-38.144501	-1.858715	1.626560	0.007176	0.705526
-38.157962	-1.854015	1.631565	0.007178	0.705530
-38.518208	-1.793789	1.636570	0.007245	0.705523
-37.996305	-1.881137	1.641574	0.007148	0.705534
-38.386533	-1.815993	1.646579	0.007221	0.705526
-38.486444	-1.882615	1.651584	0.007239	0.705356
-38.918390	-1.874262	1.656589	0.007319	0.705218
-39.271648	-1.813960	1.661594	0.007385	0.705213
-39.328819	-1.800386	1.666598	0.007396	0.705220
-39.251863	-1.817307	1.671603	0.007381	0.705213
-38.771453	-1.904085	1.676608	0.007292	0.705211
-39.018793	-1.856189	1.681613	0.007338	0.705219
-39.621382	-1.829301	1.686618	0.007450	0.705057
-40.153814	-1.815478	1.691622	0.007549	0.704894
-39.881572	-1.868175	1.696627	0.007498	0.704886
-40.251779	-1.800665	1.701632	0.007567	0.704889
-39.790818	-1.880995	1.706637	0.007481	0.704893
-39.824515	-1.878696	1.711642	0.007487	0.704886
-39.890064	-1.863785	1.716646	0.007499	0.704893
-40.218286	-1.869067	1.721651	0.007560	0.704764
-41.022985	-1.811285	1.726656	0.007710	0.704592
-40.729688	-1.860415	1.731661	0.007655	0.704598
-41.137824	-1.792805	1.736666	0.007731	0.704588
-40.760103	-1.855783	1.741670	0.007660	0.704597
-40.929576	-1.829280	1.746675	0.007692	0.704590
-41.169223	-1.784616	1.751680	0.007736	0.704594
-40.857565	-1.881276	1.756685	0.007678	0.704511
-41.699997	-1.857722	1.761690	0.007835	0.704256
-41.758746	-1.841510	1.766694	0.007846	0.704268
-42.026195	-1.797850	1.771699	0.007896	0.704260
-41.680868	-1.860980	1.776704	0.007831	0.704257
-41.242437	-1.935790	1.781709	0.007749	0.704264
-42.062187	-1.793760	1.786714	0.007902	0.704256
-41.859114	-1.882074	1.791718	0.007864	0.704151
-42.671627	-1.837244	1.796723	0.008015	0.703950
-42.563354	-1.857074	1.801728	0.007995	0.703949
-42.492171	-1.866463	1.806733	0.007982	0.703956
-42.614220	-1.848873	1.811738	0.008004	0.703948
-42.664226	-1.835228	1.816742	0.008013	0.703957
-42.677516	-1.837257	1.821747	0.008016	0.703949
-42.635340	-1.916168	1.826752	0.008008	0.703805
-43.700352	-1.808642	1.831757	0.008206	0.703639
-43.745754	-1.804520	1.836762	0.008214	0.703631
-43.452586	-1.853094	1.841766	0.008160	0.703639
-43.500758	-1.848826	1.846771	0.008168	0.703630
-43.688511	-1.812175	1.851776	0.008203	0.703637
-43.571854	-1.831914	1.856781	0.008181	0.703639
-43.559017	-1.868602	1.861786	0.008179	0.703570
-44.181907	-1.866643	1.866790	0.008295	0.703350
-44.525568	-1.810626	1.871795	0.008359	0.703340
-44.831685	-1.755930	1.876800	0.008416	0.703340
-44.228663	-1.860785	1.881805	0.008303	0.703346
-44.531739	-1.811462	1.886810	0.008360	0.703336
-44.320455	-1.845056	1.891814	0.008320	0.703345
-44.327238	-1.875951	1.896819	0.008321	0.703280
-45.146661	-1.865796	1.901824	0.008474	0.703006
-45.095532	-1.873470	1.906829	0.008464	0.703009
-45.161583	-1.866782	1.911834	0.008476	0.702999
-45.329811	-1.832146	1.916838	0.008508	0.703008
-45.533951	-1.797983	1.921843	0.008545	0.703004
-45.370401	-1.825543	1.926848	0.008515	0.703008
-44.973724	-1.942561	1.931853	0.008441	0.702914
-46.417652	-1.796712	1.936858	0.008710	0.702689
-46.233973	-1.825198	1.941862	0.008675	0.702698
-46.262881	-1.821268	1.946867	0.008681	0.702696
-46.232294	-1.825667	1.951872	0.008675	0.702698
-46.063709	-1.853662	1.956877	0.008643	0.702702
-46.338972	-1.809174	1.961882	0.008694	0.702693
-46.331351	-1.811641	1.966886	0.008693	0.702691
-46.858159	-1.875910	1.971891	0.008791	0.702372
-47.241769	-1.809595	1.976896	0.008862	0.702368
-46.952127	-1.857707	1.981901	0.008808	0.702375
-46.890924	-1.874125	1.986906	0.008797	0.702364
-46.875971	-1.871762	1.991910	0.008794	0.702374
-46.836132	-1.881824	1.996915	0.008786	0.702369
-47.327269	-1.881410	2.001920	0.008878	0.702193

-47.867403	-1.845858	2.011917	0.008978	0.702070
-47.892300	-1.839426	2.021914	0.008982	0.702075
-47.848252	-1.846366	2.031910	0.008974	0.702077
-47.924269	-1.833100	2.041907	0.008988	0.702077
-48.025089	-1.815720	2.051904	0.009006	0.702076
-47.811403	-1.855530	2.061901	0.008966	0.702073
-47.938870	-1.833902	2.071898	0.008990	0.702071
-47.920050	-1.836268	2.081894	0.008986	0.702073
-47.987730	-1.823444	2.091891	0.008999	0.702075
-48.086156	-1.806492	2.101888	0.009017	0.702075
-47.884807	-1.783647	2.111885	0.008979	0.702194
-47.059376	-1.843339	2.121882	0.008825	0.702371
-47.103290	-1.834520	2.131878	0.008833	0.702374
-47.111103	-1.832756	2.141875	0.008834	0.702375
-47.116968	-1.832150	2.151872	0.008835	0.702374
-47.086026	-1.838145	2.161869	0.008829	0.702374
-46.839143	-1.771170	2.171866	0.008783	0.702599
-46.332301	-1.813873	2.181862	0.008688	0.702695
-46.154566	-1.845109	2.191859	0.008655	0.702697
-46.224617	-1.832249	2.201856	0.008668	0.702698
-46.101263	-1.801824	2.211853	0.008645	0.702804
-45.215067	-1.860078	2.221850	0.008480	0.703006
-45.238769	-1.855133	2.231846	0.008484	0.703008
-45.517319	-1.805221	2.241843	0.008535	0.703009
-45.220449	-1.820326	2.251840	0.008480	0.703086
-44.530806	-1.816795	2.261837	0.008351	0.703342
-44.683203	-1.790495	2.271834	0.008379	0.703340
-44.474358	-1.825881	2.281830	0.008340	0.703344
-44.066348	-1.817465	2.291827	0.008264	0.703509
-43.430749	-1.866092	2.301824	0.008146	0.703640
-43.610812	-1.835015	2.311821	0.008179	0.703638
-43.482690	-1.858101	2.321818	0.008155	0.703638
-43.098492	-1.815660	2.331814	0.008083	0.703862
-43.033995	-1.780810	2.341811	0.008071	0.703956
-42.609774	-1.857257	2.351808	0.007992	0.703955
-42.751595	-1.795888	2.361805	0.008018	0.704028
-42.074987	-1.802056	2.371802	0.007892	0.704259
-41.945592	-1.824631	2.381798	0.007867	0.704261
-41.887567	-1.834833	2.391795	0.007856	0.704262
-41.198338	-1.830027	2.401792	0.007728	0.704519
-41.244779	-1.785670	2.411789	0.007736	0.704592
-40.998558	-1.829339	2.421786	0.007690	0.704593
-40.932577	-1.797765	2.431782	0.007678	0.704681
-40.151011	-1.833462	2.441779	0.007532	0.704890
-40.016612	-1.855919	2.451776	0.007507	0.704894
-40.266406	-1.812379	2.461773	0.007553	0.704892
-39.473694	-1.837960	2.471770	0.007405	0.705126
-39.284618	-1.827632	2.481766	0.007370	0.705215
-39.434757	-1.802011	2.491763	0.007397	0.705213
-38.959221	-1.865051	2.501760	0.007309	0.705257
-38.695257	-1.777649	2.511757	0.007259	0.705528
-38.450412	-1.823438	2.521754	0.007213	0.705524
-38.365670	-1.838401	2.531750	0.007197	0.705525
-37.918142	-1.791275	2.541747	0.007114	0.705781
-37.534627	-1.817732	2.551744	0.007042	0.705865
-37.411360	-1.840415	2.561741	0.007019	0.705864
-37.453458	-1.812493	2.571738	0.007027	0.705906
-36.646411	-1.845264	2.581734	0.006876	0.706130
-36.817784	-1.812480	2.591731	0.006908	0.706135
-36.642793	-1.843682	2.601728	0.006875	0.706135
-36.441417	-1.759292	2.611725	0.006837	0.706377
-35.985839	-1.806951	2.621722	0.006752	0.706445
-35.886072	-1.825756	2.631718	0.006734	0.706444
-35.560924	-1.807937	2.641715	0.006673	0.706596
-34.937355	-1.841028	2.651712	0.006556	0.706753
-35.153803	-1.802894	2.661709	0.006597	0.706753
-34.911128	-1.838767	2.671706	0.006551	0.706768
-34.280506	-1.795000	2.681702	0.006433	0.707082
-34.032317	-1.838778	2.691699	0.006387	0.707084
-33.944536	-1.854435	2.701696	0.006371	0.707084
-33.947916	-1.772971	2.711693	0.006371	0.707247
-33.080567	-1.864260	2.721690	0.006209	0.707374
-33.433360	-1.798754	2.731686	0.006275	0.707380
-33.147142	-1.834863	2.741683	0.006221	0.707410
-32.583287	-1.789912	2.751680	0.006116	0.707703
-32.293489	-1.842699	2.761677	0.006062	0.707701
-32.202557	-1.859384	2.771674	0.006045	0.707700
-32.130596	-1.778689	2.781670	0.006031	0.707888
-31.418391	-1.841405	2.791667	0.005898	0.708017
-31.434838	-1.837786	2.801664	0.005901	0.708019
-31.444300	-1.828553	2.811661	0.005903	0.708035
-30.757271	-1.791884	2.821658	0.005774	0.708354
-30.516502	-1.834880	2.831654	0.005729	0.708354
-30.505205	-1.835970	2.841651	0.005727	0.708357
-30.245453	-1.803466	2.851648	0.005678	0.708515
-29.736657	-1.830261	2.861645	0.005584	0.708643
-29.739039	-1.829810	2.871642	0.005584	0.708644
-29.821784	-1.798891	2.881638	0.005599	0.708677
-28.852771	-1.829054	2.891635	0.005418	0.708963
-28.888575	-1.823311	2.901632	0.005425	0.708962
-28.796828	-1.840258	2.911629	0.005407	0.708961
-28.443401	-1.818401	2.921626	0.005341	0.709131
-28.007114	-1.826357	2.931622	0.005260	0.709271
-28.028686	-1.822604	2.941619	0.005264	0.709272
-28.069474	-1.791259	2.951616	0.005271	0.709320
-27.183915	-1.807268	2.961613	0.005106	0.709604
-27.065868	-1.829799	2.971610	0.005084	0.709602
-27.003906	-1.842571	2.981606	0.005072	0.709599
-26.626698	-1.825806	2.991603	0.005002	0.709767
-26.221199	-1.832310	3.001600	0.004926	0.709899
-26.112439	-1.850841	3.011597	0.004905	0.709901
-26.116384	-1.851675	3.021594	0.004906	0.709898
-25.504252	-1.802143	3.031590	0.004792	0.710216
-25.188638	-1.854285	3.041587	0.004733	0.710225
-25.237151	-1.845576	3.051584	0.004742	0.710225
-25.169577	-1.795264	3.061581	0.004729	0.710350
-24.386274	-1.842896	3.071578	0.004583	0.710534
-24.352006	-1.848231	3.081574	0.004576	0.710536
-24.276017	-1.861665	3.091571	0.004562	0.710537
-23.796279	-1.802517	3.101568	0.004472	0.710826
-23.355709	-1.854610	3.111565	0.004390	0.710879
-23.525857	-1.826029	3.121562	0.004421	0.710876
-23.478844	-1.800448	3.131558	0.004412	0.710945
-22.687845	-1.841456	3.141555	0.004265	0.711144
-22.931513	-1.796411	3.151552	0.004310	0.711148
-22.645553	-1.849641	3.161549	0.004257	0.711144
-22.108503	-1.791249	3.171546	0.004156	0.711452
-21.686539	-1.862678	3.181542	0.004078	0.711460
-21.760209	-1.847332	3.191539	0.004091	0.711465
-21.646622	-1.796680	3.201536	0.004070	0.711606
-20.855672	-1.854190	3.211533	0.003922	0.711773
-21.106029	-1.811480	3.221530	0.003969	0.711770
-21.031057	-1.810311	3.231526	0.003954	0.711799
-20.276708	-1.793967	3.241523	0.003814	0.712100
-20.030246	-1.838279	3.251520	0.003768	0.712100
-20.093724	-1.826864	3.261517	0.003779	0.712100
-19.693182	-1.800796	3.271514	0.003704	0.712295
-19.185171	-1.839855	3.281510	0.003610	0.712398
-19.290065	-1.820827	3.291507	0.003629	0.712399
-19.082969	-1.834434	3.301504	0.003590	0.712446
-18.320839	-1.833610	3.311501	0.003448	0.712718
-18.247260	-1.847318	3.321498	0.003434	0.712718
-18.194162	-1.858829	3.331494	0.003424	0.712714
-18.093065	-1.788432	3.341491	0.003405	0.712890
-17.250705	-1.866196	3.351488	0.003248	0.713035
-17.653250	-1.795715	3.361485	0.003323	0.713033
-17.420162	-1.827042	3.371482	0.003279	0.713053
-16.622715	-1.812271	3.381478	0.003130	0.713366
-16.664508	-1.804484	3.391475	0.003138	0.713367
-16.455117	-1.841600	3.401472	0.003099	0.713368
-16.097930	-1.818660	3.411469	0.003032	0.713540
-15.650255	-1.840659	3.421466	0.002948	0.713656
-15.487950	-1.869779	3.431462	0.002918	0.713656
-15.716307	-1.827895	3.441459	0.002960	0.713659
-14.903032	-1.818903	3.451456	0.002809	0.713965
-14.789763	-1.831975	3.461453	0.002787	0.713979
-14.927760	-1.810865	3.471450	0.002813	0.713973
-14.512060	-1.798347	3.481446	0.002735	0.714145
-13.833142	-1.846222	3.491443	0.002609	0.714291
-13.750204	-1.862894	3.501440	0.002593	0.714288
-13.847165	-1.845162	3.511437	0.002611	0.714289
-13.175208	-1.818640	3.521434	0.002485	0.714580
-13.077215	-1.818281	3.531430	0.002467	0.714616
-13.067680	-1.819164	3.541427	0.002465	0.714618
-12.734288	-1.812524	3.551424	0.002403	0.714749
-12.094655	-1.842466	3.561421	0.002283	0.714916
-12.102953	-1.841786	3.571418	0.002285	0.714915
-12.249619	-1.815871	3.581414	0.002312	0.714915
-11.543638	-1.794521	3.591411	0.002180	0.715208
-11.257952	-1.829702	3.601408	0.002127	0.715239
-11.302751	-1.820513	3.611405	0.002135	0.715242
-11.027578	-1.800524	3.621402	0.002083	0.715379
-10.366801	-1.830721	3.631398	0.001960	0.715553
-10.452154	-1.816791	3.641395	0.001976	0.715551
-10.347758	-1.834292	3.651392	0.001956	0.715554
-9.610480	-1.801382	3.661389	0.001819	0.715880
-9.178737	-1.874228	3.671386	0.001738	0.715888
-9.118621	-1.884196	3.681382	0.001727	0.715890
-8.895052	-1.923828	3.691379	0.001685	0.715891
-8.286718	-1.918468	3.701376	0.001571	0.716117
-8.359351	-1.894776	3.711373	0.001585	0.716138
-8.224002	-1.919287	3.721370	0.001559	0.716138
-8.377932	-1.884626	3.731366	0.001588	0.716153
-7.470483	-1.894024	3.741363	0.001418	0.716455
-7.119359	-1.956411	3.751360	0.001353	0.716455
-7.283363	-1.929265	3.761357	0.001383	0.716452
-7.390234	-1.878912	3.771354	0.001403	0.716514
-6.465282	-1.918660	3.781350	0.001230	0.716762
-6.321185	-1.943623	3.791347	0.001203	0.716764
-6.334546	-1.942004	3.801344	0.001206	0.716763
-6.247366	-1.876174	3.811341	0.001189	0.716924
-5.315611	-1.958801	3.821338	0.001016	0.717089
-5.556260	-1.914848	3.831334	0.001060	0.717092
-5.408534	-1.941720	3.841331	0.001032	0.717091
-4.904672	-1.925920	3.851328	0.000938	0.717301
-4.667960	-1.924034	3.861325	0.000894	0.717388
-4.563658	-1.944792	3.871322	0.000874	0.717384
-4.412110	-1.971514	3.881318	0.000846	0.717385
-3.715672	-1.930988	3.891315	0.000716	0.717711
-3.689027	-1.933845	3.901312	0.000711	0.717715
-3.618566	-1.947589	3.911309	0.000698	0.717713
-3.732166	-1.873606	3.921306	0.000718	0.717820
-2.844831	-1.928389	3.931302	0.000553	0.718024
-2.669017	-1.960143	3.941299	0.000520	0.718024
-2.856033	-1.925663	3.951296	0.000555	0.718026
-2.212489	-1.898348	3.961293	0.000435	0.718307
-2.117584	-1.888749	3.971290	0.000417	0.718360
-1.923192	-1.922228	3.981286	0.000380	0.718363
-1.872546	-1.876888	3.991283	0.000371	0.718470
-1.619208	-1.831931	4.001280	0.000323	0.718649
-1.465178	-1.859329	4.011277	0.000294	0.718649
-1.778585	-1.743044	4.021274	0.000352	0.718769
-1.299517	-1.731075	4.031270	0.000263	0.718961
-1.086434	-1.766810	4.041267	0.000223	0.718966
-1.197604	-1.618656	4.051264	0.000244	0.719220
-0.975574	-1.628964	4.061261	0.000202	0.719278
-1.044821	-1.533714	4.071258	0.000215	0.719442
-0.844918	-1.485973	4.081254	0.000177	0.719607
-0.626954	-1.457206	4.091251	0.000136	0.719740
-1.120230	-1.284776	4.101248	0.000228	0.719907
-0.835425	-1.231591	4.111245	0.000175	0.720113
-0.747830	-1.186545	4.121242	0.000158	0.720232
-0.787205	-1.028724	4.131238	0.000165	0.720530
-0.543989	-0.999362	4.141235	0.000119	0.720673
-0.389287	-0.917260	4.151232	0.000090	0.720890
-0.487174	-0.797382	4.161229	0.000108	0.721092
-0.396555	-0.729749	4.171226	0.000091	0.721257
-0.266923	-0.652074	4.181222	0.000067	0.721455
-0.216278	-0.510499	4.191219	0.000057	0.721752
-0.267958	-0.380114	4.201216	0.000066	0.721990
-0.287775	-0.256396	4.211213	0.000070	0.722227
-0.212870	-0.144368	4.221210	0.000056	0.722474
-0.367602	0.026696	4.231206	0.000084	0.722756
-0.087560	0.120340	4.241203	0.000032	0.723038
0.000000	0.317246	4.251200	0.000015	0.723455

-0.077697	0.957607	4.256205	0.000029	0.724683
0.095400	2.181674	4.261210	-0.000004	0.727136
0.404101	3.989029	4.266214	-0.000063	0.730761
0.747947	6.337247	4.271219	-0.000129	0.735424
1.144172	9.189368	4.276224	-0.000204	0.741041
1.416378	12.551821	4.281229	-0.000257	0.747543
1.813954	16.333488	4.286234	-0.000334	0.754819
2.308749	20.517331	4.291238	-0.000429	0.762806
2.516994	25.144222	4.296243	-0.000471	0.771431
3.125751	30.067459	4.301248	-0.000588	0.780629
3.806748	35.337489	4.306253	-0.000718	0.790365
4.010937	40.997922	4.311258	-0.000760	0.800525
4.378535	46.941094	4.316262	-0.000832	0.811103
4.869934	53.131779	4.321267	-0.000928	0.822010
5.426217	59.597472	4.326272	-0.001036	0.833261
7.054824	66.087569	4.331277	-0.001343	0.844720
9.076709	72.767767	4.336282	-0.001724	0.856455
9.993931	79.868406	4.341286	-0.001900	0.868400
10.664782	87.189541	4.346291	-0.002030	0.880467
11.761756	94.624693	4.351296	-0.002239	0.892671
12.626425	102.267832	4.356301	-0.002405	0.904972
13.288164	110.086070	4.361306	-0.002533	0.917323
14.451517	117.939754	4.366310	-0.002755	0.929698
15.126345	125.976170	4.371315	-0.002886	0.942055
15.985531	134.095588	4.376320	-0.003051	0.954424
17.352480	142.203031	4.381325	-0.003311	0.966746
18.139095	150.512193	4.386330	-0.003463	0.979058
18.886948	158.918198	4.391334	-0.003608	0.991346
19.549437	167.365192	4.396339	-0.003737	1.003519
20.395544	175.833663	4.401344	-0.003900	1.015621
21.263873	184.328392	4.406349	-0.004068	1.027621
21.995376	192.882839	4.411354	-0.004210	1.039532
23.124651	201.411184	4.416358	-0.004426	1.051364
24.317716	209.945167	4.421363	-0.004653	1.063087
24.852594	218.641559	4.426368	-0.004759	1.074745
25.548253	227.282611	4.431373	-0.004894	1.086242
26.731801	235.869746	4.436378	-0.005120	1.097657
27.748259	244.496411	4.441382	-0.005315	1.108967
28.066033	253.231874	4.446387	-0.005380	1.120149
28.752051	261.895354	4.451392	-0.005514	1.131209
29.558005	270.535075	4.456397	-0.005669	1.142157
30.481133	279.178205	4.461402	-0.005847	1.153030
31.458567	287.779364	4.466406	-0.006035	1.163761
32.080669	296.425257	4.471411	-0.006156	1.174374
32.929601	305.021274	4.476416	-0.006320	1.184879
33.802230	313.622956	4.481421	-0.006488	1.195302
34.731802	322.176339	4.486426	-0.006667	1.205589
35.681688	330.747444	4.491430	-0.006850	1.215813
36.843023	339.253496	4.496435	-0.007071	1.225918
37.911837	347.813258	4.501440	-0.007276	1.235983
38.697568	356.360851	4.506445	-0.007428	1.245898
39.108654	364.971823	4.511450	-0.007510	1.255735
39.476109	373.562300	4.516454	-0.007585	1.265463
40.099770	382.094307	4.521459	-0.007706	1.275101
41.140169	390.528362	4.526464	-0.007906	1.284635
41.893783	399.018419	4.531469	-0.008052	1.294106
42.452101	407.510360	4.536474	-0.008161	1.303475
43.068264	416.087752	4.541478	-0.008282	1.312880
43.626302	424.566076	4.546483	-0.008391	1.322101
44.267879	432.980171	4.551488	-0.008516	1.331204
45.111920	441.366113	4.556493	-0.008679	1.340251
45.784557	449.768630	4.561498	-0.008810	1.349224
46.610859	458.155293	4.566502	-0.008969	1.358148
46.961663	466.570754	4.571507	-0.009040	1.366961
47.589564	474.967981	4.576512	-0.009163	1.375746
48.187829	483.334273	4.581517	-0.009280	1.384439
48.914796	491.697041	4.586522	-0.009421	1.393095
49.509606	500.053051	4.591526	-0.009537	1.401668
50.021301	508.408138	4.596531	-0.009638	1.410174
50.398955	516.794621	4.601536	-0.009714	1.418639
51.001644	525.110268	4.606541	-0.009831	1.427019
51.322927	533.487811	4.611546	-0.009897	1.435366
51.944502	541.787609	4.616550	-0.010018	1.443636
52.505276	550.099079	4.621555	-0.010128	1.451861
53.493228	558.337225	4.626560	-0.010317	1.460035
54.475398	566.593494	4.631565	-0.010506	1.468181
54.658774	575.009320	4.636570	-0.010545	1.476309
55.059942	583.298031	4.641574	-0.010626	1.484305
55.982118	591.511392	4.646579	-0.010803	1.492267
56.364996	599.818730	4.651584	-0.010880	1.500192
56.825047	608.106809	4.656589	-0.010971	1.508069
57.541372	616.346722	4.661594	-0.011110	1.515899
58.341778	624.575073	4.666598	-0.011264	1.523691
58.510936	632.891916	4.671603	-0.011301	1.531429
58.939719	641.171861	4.676608	-0.011387	1.539134
59.445817	649.416769	4.681613	-0.011486	1.546779
59.858646	657.698203	4.686618	-0.011569	1.554406
60.320163	665.927467	4.691622	-0.011660	1.561955
60.874143	674.143153	4.696627	-0.011769	1.569469
61.934212	682.296163	4.701632	-0.011971	1.576964
62.627769	690.504618	4.706637	-0.012106	1.584420
62.981457	698.770589	4.711642	-0.012177	1.591843
63.501603	707.012232	4.716646	-0.012280	1.599234
63.966256	715.223125	4.721651	-0.012372	1.606556
64.581411	723.458988	4.726656	-0.012492	1.613887
65.125231	731.669429	4.731661	-0.012598	1.621153
65.511395	739.908283	4.736666	-0.012676	1.628389
66.122698	748.164755	4.741670	-0.012795	1.635639
66.343897	756.371751	4.746675	-0.012842	1.642761
66.671299	764.576844	4.751680	-0.012908	1.649865
67.133495	772.775100	4.756685	-0.013000	1.656951
67.746486	780.910235	4.761690	-0.013119	1.663973
68.209709	789.118372	4.766694	-0.013211	1.671007
68.595404	797.317139	4.771699	-0.013288	1.677993
68.917273	805.487827	4.776704	-0.013354	1.684918
69.349828	813.694801	4.781709	-0.013440	1.691859
69.751489	821.867830	4.786714	-0.013520	1.698740
70.315179	830.033707	4.791718	-0.013630	1.705608
70.863579	838.208164	4.796723	-0.013738	1.712453
71.471104	846.361356	4.801728	-0.013856	1.719261
72.240422	854.474005	4.806733	-0.014005	1.726030
72.377180	862.702812	4.811738	-0.014036	1.732785
72.741325	870.890927	4.816742	-0.014109	1.739510
72.925949	879.077994	4.821747	-0.014149	1.746186
73.089063	887.293792	4.826752	-0.014185	1.752857
73.512424	895.444064	4.831757	-0.014269	1.759482
73.994869	903.543694	4.836762	-0.014364	1.766049
74.563671	911.708817	4.841766	-0.014476	1.772654
75.134384	919.833105	4.846771	-0.014587	1.779203
76.180632	927.898589	4.851776	-0.014787	1.785739
76.914329	936.086971	4.856781	-0.014930	1.792310
77.293226	944.270821	4.861786	-0.015005	1.798810
77.549182	952.444761	4.866790	-0.015059	1.805264
77.854823	960.607405	4.871795	-0.015121	1.811691
78.473870	968.732212	4.876800	-0.015242	1.818104
78.833785	976.880757	4.881805	-0.015314	1.824482
79.047664	985.051773	4.886810	-0.015359	1.830838
79.757010	993.161565	4.891814	-0.015497	1.837182
80.125539	1001.287306	4.896819	-0.015571	1.843477
80.580102	1009.424552	4.901824	-0.015661	1.849770
81.096638	1017.563492	4.906829	-0.015762	1.856049
81.409901	1025.709804	4.911834	-0.015826	1.862289
82.035344	1033.841079	4.916838	-0.015948	1.868533
82.166339	1042.041783	4.921843	-0.015978	1.874751
82.660245	1050.126713	4.926848	-0.016075	1.880903
83.402199	1058.212964	4.931853	-0.016219	1.887064
84.006523	1066.333861	4.936858	-0.016337	1.893215
84.308259	1074.493246	4.941862	-0.016398	1.899341
84.424039	1082.647321	4.946867	-0.016425	1.905422
84.903908	1090.771910	4.951872	-0.016520	1.911502
85.271479	1098.914819	4.956877	-0.016594	1.917564
85.544336	1107.024306	4.961882	-0.016650	1.923572
86.205456	1115.117766	4.966886	-0.016779	1.929592
86.396356	1123.270874	4.971891	-0.016820	1.935585
86.979882	1131.355161	4.976896	-0.016934	1.941552
87.569325	1139.461383	4.981901	-0.017049	1.947517
87.980672	1147.623539	4.986906	-0.017131	1.953485
88.325427	1155.746877	4.991910	-0.017200	1.959400
88.659430	1163.839682	4.996915	-0.017268	1.965274
88.931951	1171.968566	5.001920	-0.017324	1.971149
89.206858	1180.100453	5.006925	-0.017381	1.977009
89.684471	1188.181083	5.011930	-0.017475	1.982837
90.247983	1196.281921	5.016934	-0.017585	1.988671
90.788245	1204.384094	5.021939	-0.017691	1.994486
91.095371	1212.485584	5.026944	-0.017754	2.000259
91.804929	1220.551875	5.031949	-0.017891	2.006033
92.010205	1228.690122	5.036954	-0.017935	2.011788
92.323673	1236.832116	5.041958	-0.017999	2.017540
92.701453	1244.915848	5.046963	-0.018074	2.023242
93.119368	1253.018372	5.051968	-0.018158	2.028945
93.976773	1261.109761	5.056973	-0.018323	2.034669
94.492829	1269.159528	5.061978	-0.018424	2.040313
94.939068	1277.264821	5.066982	-0.018513	2.045973
95.253415	1285.389612	5.071987	-0.018577	2.051617
95.555429	1293.516388	5.076992	-0.018638	2.057246
96.191418	1301.589398	5.081997	-0.018762	2.062856
96.467504	1309.700640	5.087002	-0.018819	2.068440
96.752252	1317.848339	5.092006	-0.018877	2.074035
96.941592	1325.943837	5.097011	-0.018918	2.079571
97.356437	1334.012234	5.102016	-0.019000	2.085095
97.797003	1342.114094	5.107021	-0.019088	2.090629
98.304919	1350.200983	5.112026	-0.019188	2.096146
98.717356	1358.287459	5.117030	-0.019270	2.101638
99.093078	1366.386317	5.122035	-0.019345	2.107121
99.502406	1374.524804	5.127040	-0.019427	2.112619
99.957451	1382.623336	5.132045	-0.019517	2.118080
100.171262	1390.690211	5.137050	-0.019562	2.123483
100.364425	1398.806845	5.142054	-0.019604	2.128903
100.543239	1406.915544	5.147059	-0.019642	2.134303
101.179534	1414.946140	5.152064	-0.019766	2.139681
101.611943	1423.024226	5.157069	-0.019852	2.145057
101.640659	1431.148542	5.162074	-0.019863	2.150412
102.134220	1439.240419	5.167078	-0.019960	2.155776
102.502782	1447.298634	5.172083	-0.020034	2.161093
103.014143	1455.362655	5.177088	-0.020135	2.166414
103.585326	1463.444395	5.182093	-0.020246	2.171739
103.934394	1471.525789	5.187098	-0.020317	2.177030
104.220887	1479.629718	5.192102	-0.020376	2.182316
104.659852	1487.695038	5.197107	-0.020463	2.187579
105.095739	1495.810798	5.202112	-0.020549	2.192862
105.440280	1503.890712	5.207117	-0.020619	2.198100
105.473392	1511.991966	5.212122	-0.020630	2.203311
106.082642	1520.035810	5.217126	-0.020749	2.208525
106.420537	1528.122571	5.222131	-0.020817	2.213730
106.618425	1536.223529	5.227136	-0.020860	2.218919
106.988453	1544.289565	5.232141	-0.020934	2.224089
107.250381	1552.362956	5.237146	-0.020988	2.229242
107.741111	1560.455086	5.242150	-0.021085	2.234415
108.380440	1568.490761	5.247155	-0.021209	2.239553
108.819851	1576.544466	5.252160	-0.021296	2.244673
109.166469	1584.650394	5.257165	-0.021366	2.249807
109.942923	1592.685067	5.262170	-0.021516	2.254921
110.366026	1600.770825	5.267174	-0.021600	2.260024
110.761875	1608.850954	5.272179	-0.021679	2.265111
111.171101	1616.952950	5.277184	-0.021761	2.270200
111.374788	1625.137207	5.282189	-0.021804	2.275312
111.900780	1633.122973	5.287194	-0.021908	2.280316
112.155168	1641.204145	5.292198	-0.021960	2.285345
112.624289	1649.252059	5.297203	-0.022053	2.290361
112.860044	1657.368730	5.302208	-0.022102	2.295388
113.075625	1665.452065	5.307213	-0.022148	2.300383
113.138939	1673.524611	5.312218	-0.022165	2.305346
113.799566	1681.573781	5.317222	-0.022293	2.310335
114.247371	1689.633833	5.322227	-0.022382	2.315302
114.556312	1697.705341	5.327232	-0.022445	2.320253
114.783326	1705.778005	5.332237	-0.022493	2.325188
115.153043	1713.839341	5.337242	-0.022567	2.330117
115.474547	1721.947747	5.342246	-0.022632	2.335061
115.827252	1729.996773	5.347251	-0.022703	2.339960
116.208291	1738.045631	5.352256	-0.022779	2.344851
116.716421	1746.120073	5.357261	-0.022879	2.349758
116.900667	1754.233604	5.362266	-0.022919	2.354652
117.269441	1762.283570	5.367270	-0.022993	2.359512
117.953686	1770.257867	5.372275	-0.023126	2.364342
118.273877	1778.352216	5.377280	-0.023191	2.369205
118.580444	1786.458175	5.382285	-0.023253	2.374063
119.042196	1794.489549	5.387290	-0.023345	2.378879
119.349830	1802.552598	5.392294	-0.023407	2.383693
119.551309	1810.648967	5.397299	-0.023450	2.388507
119.948931	1818.720618	5.402304	-0.023530	2.393313
120.710755	1826.734092	5.407309	-0.023677	2.398104
121.129538	1834.766460	5.412314	-0.023760	2.402869
121.500711	1842.857255	5.417318	-0.023835	2.407655
121.823721	1850.954544	5.422323	-0.023900	2.412431
122.416943	1858.987798	5.427328	-0.024016	2.417182
122.913614	1867.046268	5.432333	-0.024114	2.421930
123.070687	1875.131663	5.437338	-0.024148	2.426658
123.553571	1883.229217	5.442342	-0.024244	2.431410
123.679514	1891.368902	5.447347	-0.024273	2.436149
124.049857	1899.367416	5.452352	-0.024347	2.440815
124.395723	1907.413042	5.457357	-0.024417	2.445498
124.529071	1915.487540	5.462362	-0.024447	2.450173
124.810668	1923.553299	5.467366	-0.024505	2.454845
125.177053	1931.597212	5.472371	-0.024578	2.459501
125.335408	1939.664412	5.477376	-0.024613	2.464147
125.566760	1947.751349	5.482381	-0.024661	2.468800
125.763078	1955.817844	5.487386	-0.024703	2.473431
126.212272	1963.844351	5.492390	-0.024792	2.478048
126.709604	1971.845083	5.497395	-0.024890	2.482646
127.085216	1979.909941	5.502400	-0.024966	2.487263
127.464695	1988.000263	5.507405	-0.025042	2.491885
127.705290	1996.073881	5.512410	-0.025092	2.496480
127.986558	2004.136036	5.517414	-0.025150	2.501062
128.391518	2012.161858	5.522419	-0.025230	2.505625
128.579816	2020.240635	5.527424	-0.025271	2.510193
128.882123	2028.366292	5.532429	-0.025332	2.514788
129.377789	2036.345141	5.537434	-0.025430	2.519305
129.723424	2044.389285	5.542438	-0.025500	2.523840
130.016712	2052.441681	5.547443	-0.025560	2.528368
130.192191	2060.530421	5.552448	-0.025598	2.532900
130.529249	2068.592487	5.557453	-0.025666	2.537420
130.609749	2076.635207	5.562458	-0.025686	2.541903
131.026826	2084.675946	5.567462	-0.025769	2.546401
131.313157	2092.740113	5.572467	-0.025828	2.550894
131.449506	2100.829458	5.577472	-0.025859	2.555383
131.937242	2108.846954	5.582477	-0.025955	2.559849
132.086400	2116.876960	5.587482	-0.025988	2.564290
132.624247	2124.933931	5.592486	-0.026093	2.568766
132.958805	2132.999286	5.597491	-0.026161	2.573224
133.403530	2141.041405	5.602496	-0.026249	2.577669
133.989082	2149.080058	5.607501	-0.026364	2.582114
134.271709	2157.132236	5.612506	-0.026422	2.586538
134.579606	2165.247299	5.617510	-0.026484	2.590990
134.884402	2173.462601	5.622515	-0.026547	2.595490
135.220211	2181.421210	5.627520	-0.026614	2.599843
135.445723	2189.447617	5.632525	-0.026662	2.604219
135.615768	2197.453355	5.637530	-0.026699	2.608573
136.019563	2205.501347	5.642534	-0.026779	2.612957
136.289378	2213.561173	5.647539	-0.026835	2.617332
136.451185	2221.596452	5.652544	-0.026870	2.621679
137.009281	2229.609104	5.657549	-0.026980	2.626033
137.165619	2237.676106	5.662554	-0.027014	2.630382
137.474089	2245.758536	5.667558	-0.027077	2.634742
137.850358	2253.759093	5.672563	-0.027152	2.639056
138.123654	2261.782367	5.677568	-0.027208	2.643367
138.558157	2269.840730	5.682573	-0.027295	2.647701
138.735009	2277.903882	5.687578	-0.027333	2.652014
139.135997	2285.975554	5.692582	-0.027413	2.656338
139.534442	2294.017448	5.697587	-0.027493	2.660640
139.778643	2302.041299	5.702592	-0.027543	2.664915
140.282862	2310.110337	5.707597	-0.027643	2.669224
140.570092	2318.190639	5.712602	-0.027702	2.673517
140.809339	2326.237857	5.717606	-0.027751	2.677783
141.011604	2334.281785	5.722611	-0.027794	2.682039
141.398605	2342.289068	5.727616	-0.027872	2.686280
141.798692	2350.322524	5.732621	-0.027952	2.690528
141.939589	2358.418492	5.737626	-0.027983	2.694787
142.280351	2366.451532	5.742630	-0.028052	2.699018
142.519565	2374.489234	5.747635	-0.028102	2.703239
142.764382	2382.505484	5.752640	-0.028153	2.707442
143.129408	2390.597276	5.757645	-0.028226	2.711685
143.644708	2398.613878	5.762650	-0.028328	2.715892
143.844987	2406.656628	5.767654	-0.028370	2.720087
144.354339	2414.681256	5.772659	-0.028470	2.724284
144.693189	2422.714051	5.777664	-0.028539	2.728469
144.873755	2430.812515	5.782669	-0.028578	2.732671
144.878517	2438.895949	5.787674	-0.028584	2.736849
145.178259	2446.934566	5.792678	-0.028645	2.741015
145.762047	2454.949738	5.797683	-0.028759	2.745180
145.665772	2463.011775	5.802688	-0.028747	2.749321
146.045723	2471.143206	5.807693	-0.028823	2.753520
146.462720	2479.150736	5.812698	-0.028906	2.757652
146.964794	2487.158745	5.817702	-0.029005	2.761783
147.191851	2495.178136	5.822707	-0.029052	2.765897
147.402818	2503.205969	5.827712	-0.029097	2.770008
147.725297	2511.294176	5.832717	-0.029162	2.774150
147.715418	2519.339343	5.837722	-0.029166	2.778245
148.123855	2527.355882	5.842726	-0.029247	2.782343
148.525238	2535.385912	5.847731	-0.029327	2.786442
148.760816	2543.421878	5.852736	-0.029376	2.790528
148.757161	2551.544895	5.857741	-0.029381	2.794638
149.111197	2559.516883	5.862746	-0.029452	2.798687
149.528428	2567.536085	5.867750	-0.029535	2.802757
149.836324	2575.580351	5.872755	-0.029598	2.806827
150.359469	2583.601264	5.877760	-0.029701	2.810893
150.821574	2591.685228	5.882765	-0.029792	2.814980
151.010036	2599.728357	5.887770	-0.029833	2.819025
151.336872	2607.758028	5.892774	-0.029899	2.823066
151.602293	2615.812001	5.897779	-0.029954	2.827109
151.750407	2623.874716	5.902784	-0.029987	2.831144
151.937561	2631.977175	5.907789	-0.030027	2.835195
152.310576	2639.960518	5.912794	-0.030102	2.839192
152.630826	2647.985787	5.917798	-0.030167	2.843201
152.910360	2656.015834	5.922803	-0.030224	2.847205
153.097578	2664.055137	5.927808	-0.030264	2.851202
153.660664	2672.112808	5.932813	-0.030374	2.855223
153.902481	2680.140484	5.937818	-0.030425	2.859206
154.090225	2688.175428	5.942822	-0.030465	2.863184
154.339943	2696.221065	5.947827	-0.030517	2.867165
154.398573	2704.277146	5.952832	-0.030533	2.871136
154.895273	2712.323579	5.957837	-0.030631	2.875120
154.954907	2720.354977	5.962842	-0.030648	2.879067
155.263879	2728.387601	5.967846	-0.030710	2.883023
155.533343	2736.435173	5.972851	-0.030766	2.886978
155.811989	2744.457148	5.977856	-0.030823	2.890916
156.352287	2752.528505	5.982861	-0.030929	2.894887
156.576634	2760.547413	5.987866	-0.030976	2.898810
156.591131	2768.622850	5.992870	-0.030984	2.902744
157.102169	2776.629680	5.997875	-0.031085	2.906665
157.239497	2784.671205	6.002880	-0.031116	2.910578
157.559134	2792.830574	6.007885	-0.031181	2.914553
157.651606	2800.798398	6.012890	-0.031203	2.918417
157.944010	2808.826731	6.017894	-0.031263	2.922317
158.473914	2816.806477	6.022899	-0.031367	2.926199
158.894645	2824.817392	6.027904	-0.031451	2.930086
159.212357	2832.901575	6.032909	-0.031515	2.933998
159.579070	2840.900522	6.037914	-0.031589	2.937866
159.986795	2848.944792	6.042918	-0.031670	2.941752
160.390982	2856.959296	6.047923	-0.031751	2.945619
160.553171	2865.016470	6.052928	-0.031786	2.949489
160.639818	2873.121811	6.057933	-0.031808	2.953373
160.843568	2881.164532	6.062938	-0.031851	2.957227
161.163040	2889.164900	6.067942	-0.031916	2.961063
161.506410	2897.164090	6.072947	-0.031985	2.964894
161.700307	2905.196320	6.077952	-0.032026	2.968728
162.100577	2913.282119	6.082957	-0.032106	2.972593
162.238890	2921.322950	6.087962	-0.032137	2.976418
162.383691	2929.362978	6.092966	-0.032170	2.980239
162.814724	2937.375850	6.097971	-0.032255	2.984056
162.905686	2945.431191	6.102976	-0.032278	2.987871
163.225660	2953.505130	6.107981	-0.032343	2.991701
163.514920	2961.537211	6.112986	-0.032402	2.995505
163.756105	2969.546925	6.117990	-0.032452	2.999292
164.045708	2977.563145	6.122995	-0.032511	3.003079
164.260692	2985.584827	6.128000	-0.032557	3.006860
164.854535	2993.616403	6.133005	-0.032673	3.010659
165.175077	3001.655632	6.138010	-0.032738	3.014444
165.191619	3009.734116	6.143014	-0.032746	3.018228
165.639697	3017.746522	6.148019	-0.032835	3.021996
165.791574	3025.763103	6.153024	-0.032868	3.025748
166.298466	3033.790476	6.158029	-0.032968	3.029517
166.459415	3041.853800	6.163034	-0.033004	3.033282
166.562304	3049.933220	6.168038	-0.033028	3.037046
166.908873	3057.935135	6.173043	-0.033098	3.040782
167.053643	3065.931463	6.178048	-0.033130	3.044500
167.461302	3073.964605	6.183053	-0.033211	3.048244
167.785568	3081.998833	6.188058	-0.033277	3.051980
168.173103	3090.048103	6.193062	-0.033355	3.055720
168.308388	3098.100693	6.198067	-0.033385	3.059446
168.632310	3106.120964	6.203072	-0.033451	3.063161
169.064001	3114.170713	6.208077	-0.033537	3.066891
169.185614	3122.203536	6.213082	-0.033565	3.070593
169.505287	3130.322602	6.218086	-0.033630	3.074340
169.861862	3138.332341	6.223091	-0.033701	3.078033
170.203331	3146.313217	6.228096	-0.033770	3.081709
170.641693	3154.305656	6.233101	-0.033857	3.085389
171.003856	3162.313469	6.238106	-0.033930	3.089069
171.373547	3170.359671	6.243110	-0.034004	3.092762
171.689786	3178.430615	6.248115	-0.034068	3.096459
171.888585	3186.447013	6.253120	-0.034111	3.100122
172.113584	3194.504016	6.258125	-0.034158	3.103800
172.175477	3202.537440	6.263130	-0.034175	3.107455
172.657643	3210.555880	6.268134	-0.034270	3.111119
172.908824	3218.628924	6.273139	-0.034322	3.114792
173.050911	3226.632088	6.278144	-0.034354	3.118425
173.528424	3234.647493	6.283149	-0.034448	3.122073
173.733084	3242.658593	6.288154	-0.034491	3.125703
173.782004	3250.715859	6.293158	-0.034506	3.129343
173.928599	3258.781972	6.298163	-0.034539	3.132987
174.298326	3266.814240	6.303168	-0.034613	3.136622
174.527494	3274.844045	6.308173	-0.034661	3.140245
174.739516	3282.855027	6.313178	-0.034706	3.143854
175.010799	3290.877224	6.318182	-0.034761	3.147467
175.454129	3298.935989	6.323187	-0.034849	3.151099
175.479135	3306.991767	6.328192	-0.034859	3.154708
175.801739	3315.021754	6.333197	-0.034925	3.158314
176.093706	3323.021394	6.338202	-0.034984	3.161901
176.264162	3331.040563	6.343206	-0.035022	3.165487
176.507742	3339.080818	6.348211	-0.035072	3.169082
176.873724	3347.105273	6.353216	-0.035146	3.172670
177.074643	3355.174455	6.358221	-0.035189	3.176268
177.437488	3363.167128	6.363226	-0.035261	3.179834
177.764219	3371.185777	6.368230	-0.035328	3.183406
177.984350	3379.263903	6.373235	-0.035374	3.186996
178.068403	3387.279499	6.378240	-0.035395	3.190549
178.601875	3395.321581	6.383245	-0.035500	3.194128
178.850424	3403.341883	6.388250	-0.035551	3.197681
179.062588	3411.368296	6.393254	-0.035596	3.201232
179.337553	3419.390032	6.398259	-0.035653	3.204779
179.560121	3427.404432	6.403264	-0.035699	3.208317
179.965340	3435.457568	6.408269	-0.035780	3.211875
179.962698	3443.511744	6.413274	-0.035785	3.215414
180.133001	3451.537312	6.418278	-0.035822	3.218942
180.370057	3459.577681	6.423283	-0.035872	3.222477
180.640550	3467.586086	6.428288	-0.035927	3.225994
180.990743	3475.626697	6.433293	-0.035998	3.229525
181.207099	3483.679370	6.438298	-0.036043	3.233052
181.546634	3491.737459	6.443302	-0.036112	3.236582
181.672832	3499.740329	6.448307	-0.036141	3.240076
182.004562	3507.704327	6.453312	-0.036208	3.243558
182.239592	3515.739776	6.458317	-0.036257	3.247062
182.234688	3523.774351	6.463322	-0.036261	3.250553
182.449063	3531.842888	6.468326	-0.036307	3.254064
182.804023	3539.898798	6.473331	-0.036378	3.257571
183.002846	3547.893383	6.478336	-0.036421	3.261041
183.257690	3555.896561	6.483341	-0.036473	3.264514
183.520097	3563.951074	6.488346	-0.036528	3.268005
183.771945	3571.994308	6.493350	-0.036580	3.271488
183.983099	3580.032526	6.498355	-0.036624	3.274962
184.448457	3587.999252	6.503360	-0.036716	3.278413
184.992460	3596.048844	6.508365	-0.036823	3.281898
185.159015	3604.059675	6.513370	-0.036859	3.285348
185.505314	3612.101511	6.518374	-0.036929	3.288814
185.825714	3620.162327	6.523379	-0.036994	3.292285
185.780609	3628.185591	6.528384	-0.036991	3.295721
185.983645	3636.230221	6.533389	-0.037034	3.299172
186.328760	3644.224781	6.538394	-0.037104	3.302604
186.650343	3652.235760	6.543398	-0.037169	3.306038
186.848805	3660.296097	6.548403	-0.037211	3.309485
186.855265	3668.351051	6.553408	-0.037218	3.312919
187.266926	3676.427230	6.558413	-0.037300	3.316374
187.276459	3684.393776	6.563418	-0.037307	3.319763
187.719457	3692.375445	6.568422	-0.037395	3.323171
188.117149	3700.426872	6.573427	-0.037474	3.326604
188.246572	3708.436487	6.578432	-0.037504	3.330005
188.738233	3716.492978	6.583437	-0.037601	3.333436
188.776610	3724.523446	6.588442	-0.037613	3.336836
189.103219	3732.524673	6.593446	-0.037679	3.340231
189.372643	3740.572414	6.598451	-0.037735	3.343639
189.684668	3748.597448	6.603456	-0.037798	3.347036
190.345780	3756.623822	6.608461	-0.037927	3.350443
190.562041	3764.677475	6.613466	-0.037972	3.353842
190.437613	3772.743993	6.618470	-0.037954	3.357230
190.806652	3780.740883	6.623475	-0.038029	3.360603
190.836525	3788.749520	6.628480	-0.038039	3.363966
191.231828	3796.772448	6.633485	-0.038118	3.367344
191.275846	3804.815454	6.638490	-0.038132	3.370715
191.611879	3812.844877	6.643494	-0.038200	3.374087
192.079249	3820.872934	6.648499	-0.038292	3.377460
191.989265	3828.881282	6.653504	-0.038281	3.380801
192.686358	3836.889941	6.658509	-0.038416	3.384167
192.827324	3844.951168	6.663514	-0.038447	3.387532
192.931907	3852.984513	6.668518	-0.038472	3.390881
193.046005	3861.128688	6.673523	-0.038499	3.394273
193.372167	3869.077807	6.678528	-0.038565	3.397587
193.671105	3877.058171	6.683533	-0.038626	3.400911
194.005455	3885.033020	6.688538	-0.038694	3.404230
194.173676	3893.099622	6.693542	-0.038730	3.407578
194.474745	3901.140681	6.698547	-0.038792	3.410916
194.418506	3909.156390	6.703552	-0.038786	3.414229
194.941145	3917.198263	6.708557	-0.038889	3.417569
195.191824	3925.186456	6.713562	-0.038941	3.420874
195.370867	3933.218639	6.718566	-0.038980	3.424192
195.697409	3941.261125	6.723571	-0.039046	3.427516
195.913906	3949.284825	6.728576	-0.039092	3.430825
196.386950	3957.308551	6.733581	-0.039185	3.434139
196.577173	3965.334934	6.738586	-0.039226	3.437442
196.862165	3973.340192	6.743590	-0.039284	3.440736
197.085262	3981.364327	6.748595	-0.039331	3.444032
197.174560	3989.404689	6.753600	-0.039353	3.447328
197.642847	3997.447714	6.758605	-0.039446	3.450634
197.910813	4005.481782	6.763610	-0.039501	3.453926
198.238680	4013.508944	6.768614	-0.039567	3.457215
198.607532	4021.529175	6.773619	-0.039641	3.460498
198.658572	4029.549385	6.778624	-0.039656	3.463769
198.869487	4037.596045	6.783629	-0.039701	3.467052
198.877073	4045.651084	6.788634	-0.039707	3.470329
199.464088	4053.653656	6.793638	-0.039822	3.473600
199.713220	4061.732055	6.798643	-0.039874	3.476887
199.716431	4069.678803	6.803648	-0.039880	3.480111
200.140063	4077.710389	6.808653	-0.039964	3.483379
200.228536	4085.758027	6.813658	-0.039986	3.486640
200.408648	4093.728149	6.818662	-0.040025	3.489869
200.743127	4101.819798	6.823667	-0.040092	3.493149
201.232256	4109.832243	6.828672	-0.040189	3.496399
201.232601	4117.834222	6.833677	-0.040194	3.499627
201.267653	4125.882789	6.838682	-0.040206	3.502871
201.392053	4133.897867	6.843686	-0.040234	3.506102
201.769353	4141.911190	6.848691	-0.040310	3.509337
202.028739	4149.934072	6.853696	-0.040364	3.512569
202.294517	4157.983436	6.858701	-0.040419	3.515808
202.528663	4165.994470	6.863706	-0.040467	3.519029
202.541678	4174.014076	6.868710	-0.040475	3.522243
203.002100	4182.017447	6.873715	-0.040566	3.525461
203.289316	4190.023409	6.878720	-0.040625	3.528672
203.389277	4198.127437	6.883725	-0.040649	3.531914
203.715834	4206.132056	6.888730	-0.040715	3.535119
203.954421	4214.131866	6.893734	-0.040765	3.538317
204.151465	4222.189145	6.898739	-0.040807	3.541534
204.248286	4230.198527	6.903744	-0.040830	3.544726
204.599280	4238.268610	6.908749	-0.040901	3.547947
204.813300	4246.273785	6.913754	-0.040946	3.551135
205.143780	4254.381520	6.918758	-0.041013	3.554364
205.356893	4262.395177	6.923763	-0.041058	3.557549
205.644317	4270.345276	6.928768	-0.041117	3.560709
205.862858	4278.365181	6.933773	-0.041163	3.563891
206.085364	4286.389703	6.938778	-0.041210	3.567072
206.344256	4294.392783	6.943782	-0.041263	3.570243
206.748988	4302.450276	6.948787	-0.041344	3.573437
206.782425	4310.481030	6.953792	-0.041356	3.576607
207.180014	4318.457056	6.958797	-0.041435	3.579763
207.543432	4326.461794	6.963802	-0.041508	3.582926
207.743428	4334.491833	6.968806	-0.041551	3.586092
208.053388	4342.549016	6.973811	-0.041614	3.589268
208.329587	4350.547512	6.978816	-0.041670	3.592418
208.731685	4358.586396	6.983821	-0.041751	3.595584
208.862045	4366.601625	6.988826	-0.041780	3.598731
209.097973	4374.601332	6.993830	-0.041829	3.601872
209.395125	4382.605419	6.998835	-0.041890	3.605013
209.428833	4390.637530	7.003840	-0.041902	3.608155
209.628863	4398.736154	7.008845	-0.041944	3.611325
209.974733	4406.758206	7.013850	-0.042014	3.614467
210.078938	4414.776207	7.018854	-0.042039	3.617597
210.201219	4422.801556	7.023859	-0.042067	3.620728
210.501741	4430.771037	7.028864	-0.042128	3.623840
210.683374	4438.830381	7.033869	-0.042167	3.626980
210.833047	4446.851594	7.038874	-0.042201	3.630102
211.143330	4454.913794	7.043878	-0.042264	3.633242
211.602431	4462.950389	7.048883	-0.042355	3.636372
211.668662	4470.919443	7.053888	-0.042372	3.639464
211.952338	4478.963553	7.058893	-0.042430	3.642587
212.302726	4486.974667	7.063898	-0.042501	3.645697
212.415934	4495.017726	7.068902	-0.042527	3.648810
212.674172	4503.069242	7.073907	-0.042581	3.651928
212.846436	4511.088239	7.078912	-0.042618	3.655028
213.204985	4519.110538	7.083917	-0.042690	3.658132
213.273467	4527.125185	7.088922	-0.042708	3.661222
213.542221	4535.121116	7.093926	-0.042764	3.664308
213.712440	4543.185673	7.098931	-0.042801	3.667415
213.890733	4551.203803	7.103936	-0.042839	3.670502
214.159634	4559.255309	7.108941	-0.042895	3.673601
214.380733	4567.266431	7.113946	-0.042941	3.676681
214.561107	4575.213740	7.118950	-0.042980	3.679733
214.801468	4583.260821	7.123955	-0.043030	3.682821
215.020282	4591.236217	7.128960	-0.043076	3.685880
215.462344	4599.245450	7.133965	-0.043164	3.688954
215.595375	4607.306155	7.138970	-0.043194	3.692038
215.809526	4615.348783	7.143974	-0.043239	3.695114
216.178470	4623.380040	7.148979	-0.043313	3.698187
216.352185	4631.396295	7.153984	-0.043351	3.701247
216.671891	4639.393504	7.158989	-0.043416	3.704300
216.800458	4647.412146	7.163994	-0.043445	3.707355
216.876832	4655.454757	7.168998	-0.043465	3.710415
217.101689	4663.597378	7.174003	-0.043512	3.713514
217.396490	4671.591904	7.179008	-0.043572	3.716555
217.860756	4679.522300	7.184013	-0.043664	3.719574
218.019136	4687.541247	7.189018	-0.043699	3.722617
218.140749	4695.525424	7.194022	-0.043727	3.725643
218.246366	4703.574115	7.199027	-0.043752	3.728691
218.587551	4711.602359	7.204032	-0.043821	3.731734
218.955612	4719.638952	7.209037	-0.043894	3.734778
219.179358	4727.657288	7.214042	-0.043941	3.737810
219.366605	4735.677041	7.219046	-0.043982	3.740838
219.499748	4743.728268	7.224051	-0.044012	3.743875
219.726592	4751.722275	7.229056	-0.044059	3.746890
220.227655	4759.723483	7.234061	-0.044158	3.749911
220.266763	4767.806915	7.239066	-0.044171	3.752951
220.443314	4775.836176	7.244070	-0.044209	3.755970
220.750195	4783.829963	7.249075	-0.044271	3.758977
220.925675	4791.865717	7.254080	-0.044309	3.761994
221.060034	4799.861300	7.259085	-0.044340	3.764993
221.189740	4807.898643	7.264090	-0.044369	3.768005
221.398557	4815.908525	7.269094	-0.044413	3.771006
221.601918	4823.950282	7.274099	-0.044457	3.774016
221.708097	4832.010185	7.279104	-0.044482	3.777028
222.173204	4839.969948	7.284109	-0.044574	3.780009
222.251898	4848.008435	7.289114	-0.044594	3.783008
222.281372	4856.022707	7.294118	-0.044604	3.785994
222.646052	4864.052197	7.299123	-0.044678	3.788991
223.045793	4872.102117	7.304128	-0.044757	3.791994
223.182376	4880.128552	7.309133	-0.044788	3.794981
223.452560	4888.150257	7.314138	-0.044844	3.797966
223.628297	4896.127473	7.319142	-0.044882	3.800930
223.894845	4904.140298	7.324147	-0.044937	3.803906
223.908657	4912.168145	7.329152	-0.044945	3.806881
224.293193	4920.160809	7.334157	-0.045022	3.809848
224.480707	4928.216715	7.339162	-0.045062	3.812832
224.748368	4936.233060	7.344166	-0.045117	3.815801
224.982058	4944.277148	7.349171	-0.045166	3.818777
225.208369	4952.273874	7.354176	-0.045213	3.821733
225.453861	4960.254644	7.359181	-0.045265	3.824681
225.489395	4968.318727	7.364186	-0.045276	3.827653
225.610886	4976.307953	7.369190	-0.045304	3.830597
225.842231	4984.400837	7.374195	-0.045353	3.833579
226.003108	4992.417383	7.379200	-0.045388	3.836530
226.505111	5000.404310	7.384205	-0.045487	3.839474
226.620953	5008.435888	7.389210	-0.045514	3.842424
226.719197	5016.390358	7.394214	-0.045537	3.845343
227.078922	5024.458486	7.399219	-0.045610	3.848307
227.231963	5032.460682	7.404224	-0.045644	3.851241
227.600873	5040.531586	7.409229	-0.045718	3.854201
227.813506	5048.551549	7.414234	-0.045763	3.857138
228.081472	5056.548239	7.419238	-0.045818	3.860065
228.364845	5064.604192	7.424243	-0.045876	3.863011
228.251658	5072.584055	7.429248	-0.045860	3.865920
228.625380	5080.642455	7.434253	-0.045935	3.868865
228.864006	5088.691190	7.439258	-0.045985	3.871801
228.851167	5096.937949	7.444262	-0.045988	3.874802
229.200065	5104.850839	7.449267	-0.046058	3.877687
229.395296	5112.775272	7.454272	-0.046100	3.880570
229.605262	5120.748783	7.459277	-0.046144	3.883469
229.872075	5128.775309	7.464282	-0.046199	3.886387
230.144308	5136.773252	7.469286	-0.046255	3.889292
230.362023	5144.837877	7.474291	-0.046301	3.892218
230.618055	5152.816115	7.479296	-0.046354	3.895111
230.911038	5160.851169	7.484301	-0.046414	3.898023
231.049516	5168.867438	7.489306	-0.046445	3.900924
231.172897	5176.848144	7.494310	-0.046473	3.903809
231.360092	5184.927619	7.499315	-0.046514	3.906728
231.635037	5192.898816	7.504320	-0.046570	3.909608
231.680578	5200.970764	7.509325	-0.046584	3.912518
231.833849	5209.012123	7.514330	-0.046618	3.915417
232.022751	5216.985702	7.519334	-0.046658	3.918290
232.400152	5224.981022	7.524339	-0.046734	3.921172
232.471955	5232.960176	7.529344	-0.046753	3.924041
232.855360	5241.014183	7.534349	-0.046829	3.926939
233.263148	5248.987812	7.539354	-0.046911	3.929807
233.456462	5257.040676	7.544358	-0.046952	3.932698
233.720426	5265.103082	7.549363	-0.047007	3.935591
233.850986	5273.113470	7.554368	-0.047036	3.938461
233.998276	5281.127209	7.559373	-0.047069	3.941331
233.982604	5289.135495	7.564378	-0.047071	3.944193
234.311263	5297.187272	7.569382	-0.047138	3.947075
234.815799	5305.184175	7.574387	-0.047237	3.949938
234.926367	5313.233009	7.579392	-0.047263	3.952811
235.063589	5321.263708	7.584397	-0.047294	3.955676
235.244223	5329.264047	7.589402	-0.047333	3.958529
235.630430	5337.221085	7.594406	-0.047410	3.961367
235.691603	5345.272989	7.599411	-0.047427	3.964232
235.864879	5353.279827	7.604416	-0.047465	3.967080
236.142623	5361.282372	7.609421	-0.047522	3.969927
236.216273	5369.354789	7.614426	-0.047541	3.972793
236.568189	5377.355969	7.619430	-0.047611	3.975636
236.918798	5385.408924	7.624435	-0.047682	3.978496
236.978171	5393.406160	7.629440	-0.047699	3.981329
237.111406	5401.408415	7.634445	-0.047729	3.984162
237.499712	5409.469361	7.639450	-0.047806	3.987019
237.617501	5417.460951	7.644454	-0.047834	3.989845
237.929324	5425.539775	7.649459	-0.047897	3.992702
238.238470	5433.544986	7.654464	-0.047960	3.995532
238.426985	5441.554289	7.659469	-0.048000	3.998359
238.429188	5449.582916	7.664474	-0.048006	4.001188
238.435890	5457.576232	7.669478	-0.048013	4.004002
238.884782	5465.633002	7.674483	-0.048102	4.006844
238.837350	5473.576137	7.679488	-0.048098	4.009636
238.998046	5481.651746	7.684493	-0.048133	4.012476
239.404277	5489.688718	7.689498	-0.048214	4.015304
239.412930	5497.693481	7.694502	-0.048221	4.018112
239.521415	5505.723624	7.699507	-0.048247	4.020929
239.675566	5513.715605	7.704512	-0.048281	4.023731
239.988515	5521.726995	7.709517	-0.048344	4.026541
240.184665	5529.770488	7.714522	-0.048386	4.029358
240.239635	5537.790808	7.719526	-0.048402	4.032163
240.694400	5545.935862	7.724531	-0.048492	4.035015
240.830201	5553.893542	7.729536	-0.048523	4.037795
241.195466	5561.815909	7.734541	-0.048596	4.040564
241.518725	5569.823544	7.739546	-0.048661	4.043361
241.444183	5577.832612	7.744550	-0.048653	4.046150
241.586074	5585.876896	7.749555	-0.048685	4.048952
241.736975	5593.869001	7.754560	-0.048718	4.051735
241.983139	5601.934674	7.759565	-0.048769	4.054543
242.321535	5609.966370	7.764570	-0.048838	4.057338
242.515594	5617.896206	7.769574	-0.048879	4.060094
242.875284	5625.981530	7.774579	-0.048951	4.062904
243.032731	5633.959945	7.779584	-0.048986	4.065672
243.029262	5642.022352	7.784589	-0.048991	4.068465
243.358998	5650.035694	7.789594	-0.049057	4.071244
243.643370	5658.060948	7.794598	-0.049116	4.074025
243.736941	5666.115506	7.799603	-0.049138	4.076811
244.142682	5674.067702	7.804608	-0.049219	4.079564
244.518544	5682.076349	7.809613	-0.049295	4.082334
244.584764	5690.063564	7.814618	-0.049312	4.085091
244.666513	5698.119925	7.819622	-0.049333	4.087869
245.060821	5706.142745	7.824627	-0.049412	4.090639
245.106095	5714.186181	7.829632	-0.049425	4.093409
245.371596	5722.205936	7.834637	-0.049480	4.096172
245.638909	5730.232066	7.839642	-0.049535	4.098935
245.876882	5738.227559	7.844646	-0.049585	4.101686
246.116370	5746.239384	7.849651	-0.049635	4.104440
246.126839	5754.294250	7.854656	-0.049642	4.107204
246.549415	5762.264789	7.859661	-0.049726	4.109943
246.645597	5770.366630	7.864666	-0.049749	4.112721
247.002976	5778.378813	7.869670	-0.049821	4.115469
247.535773	5786.392929	7.874675	-0.049926	4.118218
247.816297	5794.342219	7.879680	-0.049983	4.120940
248.209520	5802.353185	7.884685	-0.050062	4.123683
248.290155	5810.420965	7.889690	-0.050082	4.126439
248.525869	5818.418260	7.894694	-0.050131	4.129172
248.747925	5826.492856	7.899699	-0.050178	4.131928
249.047310	5834.502449	7.904704	-0.050239	4.134662
249.008482	5842.554862	7.909709	-0.050237	4.137404
249.482233	5850.515134	7.914714	-0.050331	4.140120
249.693926	5858.526534	7.919718	-0.050376	4.142847
249.909281	5866.539510	7.924723	-0.050421	4.145574
250.037332	5874.578281	7.929728	-0.050450	4.148306
250.235903	5882.588762	7.934733	-0.050493	4.151028
250.446674	5890.653891	7.939738	-0.050537	4.153767
250.854646	5898.687481	7.944742	-0.050618	4.156495
251.062316	5906.673236	7.949747	-0.050662	4.159203
251.100104	5914.677252	7.954752	-0.050675	4.161913
251.362058	5922.655188	7.959757	-0.050729	4.164616
251.653851	5930.730733	7.964762	-0.050789	4.167350
251.725154	5938.687594	7.969766	-0.050807	4.170039
252.141446	5946.739361	7.974771	-0.050890	4.172763
252.168161	5954.778454	7.979776	-0.050900	4.175476
252.407158	5962.795696	7.984781	-0.050950	4.178183
252.600248	5970.800229	7.989786	-0.050991	4.180883
252.835910	5978.804983	7.994790	-0.051041	4.183581
253.008202	5986.823476	7.999795	-0.051078	4.186282
253.065072	5994.839653	8.004800	-0.051094	4.188979
253.352048	6002.914347	8.009805	-0.051153	4.191697
253.768748	6010.976506	8.014810	-0.051236	4.194409
253.800754	6018.978516	8.019814	-0.051247	4.197096
253.974406	6026.922766	8.024819	-0.051285	4.199763
254.053465	6034.939243	8.029824	-0.051305	4.202452
254.255632	6042.933003	8.034829	-0.051348	4.205133
254.356408	6050.972252	8.039834	-0.051372	4.207826
254.807720	6058.958825	8.044838	-0.051461	4.210503
254.896702	6067.029401	8.049843	-0.051483	4.213203
254.863963	6075.019015	8.054848	-0.051482	4.215873
255.141592	6083.001962	8.059853	-0.051539	4.218542
255.344828	6091.034312	8.064858	-0.051582	4.221225
255.307309	6099.012219	8.069862	-0.051581	4.223885
255.808200	6107.047440	8.074867	-0.051679	4.226569
255.951723	6115.082037	8.079872	-0.051711	4.229247
256.067729	6123.118805	8.084877	-0.051738	4.231924
256.277995	6131.156241	8.089882	-0.051783	4.234600
256.349127	6139.177305	8.094886	-0.051802	4.237268
256.673773	6147.170259	8.099891	-0.051867	4.239927
256.661495	6155.182160	8.104896	-0.051870	4.242587
256.879482	6163.154347	8.109901	-0.051916	4.245235
257.117453	6171.217703	8.114906	-0.051966	4.247911
257.205976	6179.195032	8.119910	-0.051988	4.250556
257.604450	6187.285218	8.124915	-0.052067	4.253240
257.792115	6195.320128	8.129920	-0.052108	4.255901
258.042341	6203.325500	8.134925	-0.052159	4.258552
258.195053	6211.339409	8.139930	-0.052193	4.261203
258.405281	6219.342741	8.144934	-0.052238	4.263849
258.533708	6227.378735	8.149939	-0.052267	4.266504
258.623493	6235.377228	8.154944	-0.052289	4.269144
259.013187	6243.423465	8.159949	-0.052367	4.271801
259.448883	6251.492698	8.164954	-0.052453	4.274464
259.344698	6259.505427	8.169958	-0.052439	4.277102
259.488657	6267.452546	8.174963	-0.052471	4.279719
259.844334	6275.509630	8.179968	-0.052543	4.282373
260.089168	6283.438669	8.184973	-0.052594	4.284982
260.241878	6291.543059	8.189978	-0.052628	4.287646
260.379645	6299.477912	8.194982	-0.052659	4.290252
260.650174	6307.610612	8.199987	-0.052714	4.292923
260.941616	6315.584225	8.204992	-0.052774	4.295540
260.913358	6323.595856	8.209997	-0.052774	4.298166
261.372601	6331.636620	8.215002	-0.052865	4.300803
261.285399	6339.625136	8.220006	-0.052854	4.303417
261.514393	6347.648677	8.225011	-0.052902	4.306044
261.788919	6355.664750	8.230016	-0.052958	4.308667
261.989931	6363.666407	8.235021	-0.053001	4.311283
262.295383	6371.716657	8.240026	-0.053063	4.313913
262.241167	6379.727041	8.245030	-0.053059	4.316527
262.508574	6387.741170	8.250035	-0.053114	4.319143
262.620418	6395.739599	8.255040	-0.053140	4.321751
262.750965	6403.708966	8.260045	-0.053170	4.324347
263.141035	6411.782381	8.265050	-0.053248	4.326978
263.217384	6419.779952	8.270054	-0.053267	4.329581
263.353389	6427.821503	8.275059	-0.053298	4.332196
263.404857	6435.854299	8.280064	-0.053313	4.334807
263.716952	6443.832930	8.285069	-0.053376	4.337400
264.063506	6451.846581	8.290074	-0.053446	4.340003
264.059418	6459.861439	8.295078	-0.053451	4.342603
264.361180	6467.895432	8.300083	-0.053512	4.345209
264.571296	6475.886005	8.305088	-0.053556	4.347799
264.765868	6483.878834	8.310093	-0.053598	4.350388
265.010649	6492.017446	8.315098	-0.053649	4.353023
265.035155	6500.029009	8.320102	-0.053659	4.355614
265.218932	6508.052106	8.325107	-0.053698	4.358208
265.416690	6515.987959	8.330112	-0.053741	4.360773
265.467917	6523.992146	8.335117	-0.053755	4.363357
265.665996	6531.963654	8.340122	-0.053798	4.365930
265.882149	6539.995813	8.345126	-0.053843	4.368521
266.146949	6548.073667	8.350131	-0.053898	4.371125
266.182862	6556.089584	8.355136	-0.053910	4.373707
266.358080	6564.095286	8.360141	-0.053948	4.376284
266.697115	6572.086536	8.365146	-0.054016	4.378856
267.077133	6580.060578	8.370150	-0.054092	4.381422
267.105665	6588.096722	8.375155	-0.054103	4.384004
266.951920	6596.107498	8.380160	-0.054080	4.386575
267.440098	6604.122406	8.385165	-0.054176	4.389149
267.821202	6612.197472	8.390170	-0.054252	4.391741
267.882099	6620.208401	8.395174	-0.054269	4.394309
267.943819	6628.268883	8.400179	-0.054286	4.396891
268.204752	6636.209174	8.405184	-0.054340	4.399434
268.230429	6644.237734	8.410189	-0.054350	4.402003
268.509093	6652.291679	8.415194	-0.054407	4.404580
268.742018	6660.270016	8.420198	-0.054456	4.407130
269.038578	6668.315719	8.425203	-0.054516	4.409701
268.848465	6676.320318	8.430208	-0.054486	4.412255
269.208533	6684.350176	8.435213	-0.054559	4.414818
269.405926	6692.420403	8.440218	-0.054601	4.417392
269.377762	6700.374998	8.445222	-0.054601	4.419927
269.613397	6708.424763	8.450227	-0.054650	4.422491
269.810389	6716.369913	8.455232	-0.054692	4.425021
269.895853	6724.465474	8.460237	-0.054713	4.427596
270.092920	6732.478893	8.465242	-0.054755	4.430144
270.241622	6740.500571	8.470246	-0.054788	4.432693
270.519564	6748.558770	8.475251	-0.054845	4.435253
270.667229	6756.532797	8.480256	-0.054878	4.437784
270.920696	6764.472753	8.485261	-0.054931	4.440303
270.996492	6772.553422	8.490266	-0.054950	4.442865
271.258745	6780.490723	8.495270	-0.055004	4.445380
271.587842	6788.581797	8.500275	-0.055071	4.447943
271.661266	6796.569026	8.505280	-0.055090	4.450470
271.919605	6804.651617	8.510285	-0.055143	4.453027
271.888501	6812.653177	8.515290	-0.055143	4.455556
272.095198	6820.669597	8.520294	-0.055187	4.458089
272.459845	6828.656371	8.525299	-0.055260	4.460612
272.504171	6836.678820	8.530304	-0.055274	4.463143
272.822834	6844.644658	8.535309	-0.055338	4.465656
273.062985	6852.728856	8.540314	-0.055388	4.468204
273.109737	6860.724461	8.545318	-0.055402	4.470723
273.358562	6868.778241	8.550323	-0.055454	4.473259
273.533655	6876.759959	8.555328	-0.055492	4.475771
273.651775	6884.761653	8.560333	-0.055519	4.478287
273.799209	6892.756711	8.565338	-0.055552	4.480800
274.073781	6900.767150	8.570343	-0.055609	4.483316
274.136067	6908.778040	8.575347	-0.055625	4.485831
274.337783	6916.818184	8.580352	-0.055668	4.488354
274.495742	6924.822458	8.585357	-0.055703	4.490864
274.687251	6932.881840	8.590362	-0.055744	4.493390
274.976051	6940.869311	8.595367	-0.055803	4.495892
275.272786	6948.910181	8.600371	-0.055864	4.498410
275.282543	6956.898883	8.605376	-0.055871	4.500909
275.377957	6964.913401	8.610381	-0.055894	4.503415
275.463597	6972.958480	8.615386	-0.055915	4.505929
275.598173	6980.966769	8.620391	-0.055946	4.508431
275.720694	6988.983647	8.625395	-0.055974	4.510933
275.869977	6997.048911	8.630400	-0.056007	4.513450
276.160877	7005.042754	8.635405	-0.056066	4.515943
276.401309	7013.039432	8.640410	-0.056117	4.518435
276.435790	7021.007717	8.645415	-0.056128	4.520917
276.723879	7029.041200	8.650419	-0.056187	4.523418
276.846626	7037.000831	8.655424	-0.056215	4.525894
276.846244	7045.034816	8.660429	-0.056221	4.528392
276.862151	7053.070149	8.665434	-0.056229	4.530889
277.026797	7061.110227	8.670439	-0.056265	4.533386
277.388799	7069.133790	8.675443	-0.056338	4.535877
277.393857	7077.125221	8.680448	-0.056344	4.538356
277.652247	7085.110910	8.685453	-0.056397	4.540833
277.833647	7093.176956	8.690458	-0.056437	4.543333
277.887109	7101.149193	8.695463	-0.056452	4.545802
278.164130	7109.193596	8.700467	-0.056509	4.548292
278.377338	7117.191261	8.705472	-0.056554	4.550767
278.478509	7125.267455	8.710477	-0.056578	4.553264
278.634146	7133.291380	8.715482	-0.056612	4.555744
278.816227	7141.275185	8.720487	-0.056652	4.558210
279.243164	7149.287037	8.725491	-0.056736	4.560683
279.245540	7157.296335	8.730496	-0.056742	4.563154
279.396670	7165.268133	8.735501	-0.056776	4.565613
279.664142	7173.368698	8.740506	-0.056831	4.568109
279.708841	7181.269413	8.745511	-0.056844	4.570543
279.836898	7189.358849	8.750515	-0.056874	4.573033
280.061306	7197.382586	8.755520	-0.056921	4.575502
280.212973	7205.455524	8.760525	-0.056954	4.577985
280.403386	7213.424153	8.765530	-0.056995	4.580434
280.529874	7221.460214	8.770535	-0.057024	4.582903
280.791200	7229.430395	8.775539	-0.057078	4.585350
280.763022	7237.486487	8.780544	-0.057078	4.587822
281.214003	7245.477567	8.785549	-0.057167	4.590272
281.524205	7253.555632	8.790554	-0.057230	4.592749
281.714448	7261.557637	8.795559	-0.057271	4.595200
281.916539	7269.625198	8.800563	-0.057314	4.597670
281.952689	7277.558308	8.805568	-0.057326	4.600098
282.237765	7285.591794	8.810573	-0.057385	4.602555
282.301066	7293.522217	8.815578	-0.057402	4.604979
282.615139	7301.564459	8.820583	-0.057466	4.607436
283.024443	7309.591824	8.825587	-0.057547	4.609887
282.994738	7317.709929	8.830592	-0.057547	4.612365
282.942810	7325.642959	8.835597	-0.057543	4.614785
283.234195	7333.737523	8.840602	-0.057602	4.617252
283.275929	7341.602340	8.845607	-0.057615	4.619649
283.480063	7349.707484	8.850611	-0.057659	4.622117
283.780315	7357.701358	8.855616	-0.057720	4.624550
283.828192	7365.689643	8.860621	-0.057734	4.626980
284.114599	7373.732147	8.865626	-0.057793	4.629425
284.089182	7381.732840	8.870631	-0.057793	4.631857
284.425724	7389.837633	8.875635	-0.057861	4.634318
284.382852	7397.847821	8.880640	-0.057859	4.636750
284.521467	7405.787742	8.885645	-0.057890	4.639159
284.821765	7413.798387	8.890650	-0.057951	4.641588
284.930600	7421.773418	8.895655	-0.057977	4.644005
285.037298	7429.812435	8.900659	-0.058002	4.646440
285.433812	7437.848768	8.905664	-0.058081	4.648872
285.696047	7445.866141	8.910669	-0.058135	4.651298
285.588502	7453.918014	8.915674	-0.058121	4.653734
285.595579	7461.924035	8.920679	-0.058127	4.656154
286.013208	7469.945697	8.925683	-0.058210	4.658577
286.368614	7477.922763	8.930688	-0.058282	4.660985
286.343415	7485.906084	8.935693	-0.058282	4.663395
286.560573	7493.958100	8.940698	-0.058328	4.665823
286.697436	7501.964202	8.945703	-0.058359	4.668237
287.031493	7509.970560	8.950707	-0.058427	4.670649
287.136061	7518.079252	8.955712	-0.058451	4.673091
287.360595	7526.119378	8.960717	-0.058499	4.675511
287.356467	7534.145592	8.965722	-0.058503	4.677926
287.462308	7542.017852	8.970727	-0.058528	4.680293
287.757480	7550.108508	8.975731	-0.058588	4.682724
287.995490	7558.033622	8.980736	-0.058638	4.685104
288.088690	7566.066809	8.985741	-0.058661	4.687516
288.327199	7574.074096	8.990746	-0.058710	4.689918
288.482882	7582.129695	8.995751	-0.058745	4.692334
288.592204	7590.152674	9.000755	-0.058770	4.694739
288.846530	7598.184164	9.005760	-0.058823	4.697145
288.990045	7606.138632	9.010765	-0.058855	4.699527
289.191197	7614.212469	9.015770	-0.058898	4.701943
289.334975	7622.129277	9.020775	-0.058930	4.704311
289.556386	7630.253462	9.025779	-0.058977	4.706739
289.794603	7638.231626	9.030784	-0.059026	4.709123
289.636094	7646.256125	9.035789	-0.059002	4.711520
289.866153	7654.334488	9.040794	-0.059050	4.713932
289.928546	7662.314942	9.045799	-0.059067	4.716313
290.134013	7670.293589	9.050803	-0.059111	4.718692
290.264549	7678.318524	9.055808	-0.059141	4.721083
290.530177	7686.287177	9.060813	-0.059195	4.723457
290.711233	7694.361806	9.065818	-0.059234	4.725861
290.587865	7702.398464	9.070823	-0.059217	4.728253
290.909430	7710.381138	9.075827	-0.059282	4.730627
291.003824	7718.432589	9.080832	-0.059305	4.733020
291.011220	7726.407295	9.085837	-0.059312	4.735390
291.275204	7734.448949	9.090842	-0.059366	4.737778
291.505891	7742.430208	9.095847	-0.059414	4.740147
291.641847	7750.485968	9.100851	-0.059445	4.742537
291.582633	7758.449733	9.105856	-0.059439	4.744899
291.799269	7766.500973	9.110861	-0.059485	4.747285
292.260112	7774.496228	9.115866	-0.059576	4.749652
292.231183	7782.527284	9.120871	-0.059576	4.752030
292.345515	7790.615941	9.125875	-0.059603	4.754424
292.657983	7798.630087	9.130880	-0.059666	4.756793
292.998367	7806.565301	9.135885	-0.059735	4.759138
292.941062	7814.597378	9.140890	-0.059730	4.761512
293.196405	7822.547942	9.145895	-0.059782	4.763860
293.301916	7830.567054	9.150899	-0.059807	4.766227
293.445796	7838.634139	9.155904	-0.059840	4.768607
293.600523	7846.626067	9.160909	-0.059874	4.770963
293.788238	7854.744320	9.165914	-0.059914	4.773355
293.938159	7862.679631	9.170919	-0.059947	4.775693
294.308967	7870.717664	9.175923	-0.060022	4.778058
294.351413	7878.708129	9.180928	-0.060035	4.780410
294.343242	7886.744225	9.185933	-0.060039	4.782775
294.804837	7894.719461	9.190938	-0.060130	4.785118
294.804926	7902.723334	9.195943	-0.060135	4.787470
295.012226	7910.732359	9.200947	-0.060179	4.789822
295.115627	7918.792639	9.205952	-0.060204	4.792188
295.271947	7926.808876	9.210957	-0.060238	4.794540
295.387456	7934.830567	9.215962	-0.060265	4.796892
295.605428	7942.791938	9.220967	-0.060311	4.799225
295.700255	7950.816981	9.225971	-0.060334	4.801577
296.196563	7958.859330	9.230976	-0.060432	4.803930
296.294823	7966.839136	9.235981	-0.060455	4.806265
296.408384	7974.893577	9.240986	-0.060482	4.808621
296.642405	7982.858073	9.245991	-0.060531	4.810949
296.797300	7990.300577	9.250995	-0.060564	4.813124
296.866315	7994.809397	9.256000	-0.060580	4.814441

297.036711	7997.344083	9.261005	-0.060614	4.815181
297.229416	7998.722030	9.266010	-0.060651	4.815582
297.182000	7999.138015	9.271015	-0.060642	4.815704
297.353058	8000.151230	9.276019	-0.060675	4.815999
297.545397	8000.218892	9.281024	-0.060711	4.816018
297.664906	8000.218950	9.286029	-0.060733	4.816017
297.509372	8000.230013	9.291034	-0.060704	4.816021
297.697740	8000.197125	9.296039	-0.060740	4.816011
297.943670	8000.193081	9.301043	-0.060785	4.816008
297.979941	8000.232236	9.306048	-0.060792	4.816020
298.022188	8000.203089	9.311053	-0.060800	4.816011
298.109658	8000.217527	9.316058	-0.060817	4.816015
298.207281	8000.197944	9.321063	-0.060835	4.816008
298.201308	8000.240603	9.326067	-0.060834	4.816021
298.259693	8000.249164	9.331072	-0.060845	4.816023
298.433383	8000.180733	9.336077	-0.060877	4.816002
298.428963	8000.251212	9.341082	-0.060877	4.816023
298.477239	8000.251037	9.346087	-0.060886	4.816022
298.404098	8000.232607	9.351091	-0.060872	4.816017
298.515740	8000.294520	9.356096	-0.060893	4.816035
298.624493	8000.276211	9.361101	-0.060914	4.816029
298.728516	8000.314468	9.366106	-0.060933	4.816040
298.952276	8000.207402	9.371111	-0.060975	4.816007
298.881189	8000.200768	9.376115	-0.060962	4.816005
298.958281	8000.223568	9.381120	-0.060976	4.816012
299.064725	8000.176354	9.386125	-0.060996	4.815997
299.073044	8000.259895	9.391130	-0.060998	4.816022
299.089862	8000.243110	9.396135	-0.061001	4.816017
299.088600	8000.219581	9.401139	-0.061001	4.816010
299.142542	8000.299681	9.406144	-0.061011	4.816033
299.123093	8000.248026	9.411149	-0.061007	4.816018
299.215405	8000.248657	9.416154	-0.061025	4.816018
299.074732	8000.183025	9.421159	-0.060999	4.815999
299.245759	8000.194717	9.426163	-0.061031	4.816002
299.211452	8000.218686	9.431168	-0.061024	4.816009
299.342449	8000.184749	9.436173	-0.061049	4.815998
299.300216	8000.250262	9.441178	-0.061041	4.816018
299.357141	8000.256659	9.446183	-0.061052	4.816019
299.472088	8000.175394	9.451187	-0.061073	4.815995
299.404968	8000.255417	9.456192	-0.061061	4.816019
299.348592	8000.244776	9.461197	-0.061051	4.816016
299.294623	8000.265178	9.466202	-0.061041	4.816022
299.543513	8000.186364	9.471207	-0.061087	4.815998
299.507286	8000.197471	9.476211	-0.061080	4.816001
299.399097	8000.214743	9.481216	-0.061060	4.816007
299.467548	8000.191420	9.486221	-0.061073	4.816000
299.649102	8000.174443	9.491226	-0.061107	4.815994
299.755071	8000.233047	9.496231	-0.061127	4.816010
299.758083	8000.208527	9.501235	-0.061128	4.816003
299.622930	8000.264858	9.506240	-0.061103	4.816020
299.718712	8000.262345	9.511245	-0.061121	4.816019
299.666045	8000.299875	9.516250	-0.061111	4.816030
299.698577	8000.276964	9.521255	-0.061117	4.816023
299.474513	8000.294253	9.526259	-0.061075	4.816030
299.552795	8000.291421	9.531264	-0.061090	4.816028
299.738121	8000.281995	9.536269	-0.061125	4.816025
299.772614	8000.275155	9.541274	-0.061131	4.816022
299.543127	8000.247448	9.546279	-0.061089	4.816015
299.890973	8000.286963	9.551283	-0.061154	4.816025
299.905149	8000.269060	9.556288	-0.061156	4.816020
299.732292	8000.162218	9.561293	-0.061124	4.815990
299.794493	8000.225367	9.566298	-0.061136	4.816008
299.783011	8000.240133	9.571303	-0.061134	4.816012
300.026973	8000.199712	9.576307	-0.061179	4.815999
300.063498	8000.270943	9.581312	-0.061186	4.816020
299.823547	8000.119045	9.586317	-0.061142	4.815976
299.908959	8000.257446	9.591322	-0.061158	4.816016
299.853792	8000.223309	9.596327	-0.061148	4.816007
299.789748	8000.165493	9.601331	-0.061136	4.815990
300.034144	8000.218079	9.606336	-0.061181	4.816004
299.876249	8000.177787	9.611341	-0.061152	4.815993
300.027893	8000.262883	9.616346	-0.061180	4.816017
299.918757	8000.228828	9.621351	-0.061160	4.816008
300.075113	8000.195355	9.626355	-0.061189	4.815997
300.148961	8000.261925	9.631360	-0.061203	4.816016
300.168399	8000.207773	9.636365	-0.061207	4.816000
300.143276	8000.272532	9.641370	-0.061202	4.816020
300.188618	8000.264820	9.646375	-0.061211	4.816017
300.227220	8000.251641	9.651379	-0.061218	4.816013
300.346721	8000.291253	9.656384	-0.061241	4.816024
300.133768	8000.262780	9.661389	-0.061201	4.816017
300.251604	8000.246774	9.666394	-0.061223	4.816011
300.426627	8000.231816	9.671399	-0.061256	4.816006
300.300025	8000.202785	9.676403	-0.061232	4.815998
300.247306	8000.247797	9.681408	-0.061223	4.816012
300.365479	8000.262798	9.686413	-0.061245	4.816015
300.527703	8000.266848	9.691418	-0.061275	4.816016
300.401547	8000.267756	9.696423	-0.061252	4.816017
300.284237	8000.226067	9.701427	-0.061230	4.816005
300.284563	8000.250670	9.706432	-0.061230	4.816012
300.487088	8000.214836	9.711437	-0.061268	4.816001
300.531458	8000.297971	9.716442	-0.061276	4.816025
300.378910	8000.249222	9.721447	-0.061248	4.816011
300.448200	8000.263329	9.726451	-0.061261	4.816015
300.306169	8000.286396	9.731456	-0.061235	4.816023
300.454059	8000.223905	9.736461	-0.061262	4.816004
300.613806	8000.269600	9.741466	-0.061292	4.816016
300.364660	8000.289636	9.746471	-0.061246	4.816023
300.316799	8000.286633	9.751475	-0.061237	4.816023
300.324328	8000.303885	9.756480	-0.061239	4.816028
300.520836	8000.265803	9.761485	-0.061275	4.816015
300.392004	8000.305146	9.766490	-0.061252	4.816028
300.423881	8000.282222	9.771495	-0.061258	4.816021
300.320411	8000.231165	9.776499	-0.061238	4.816006
300.411822	8000.324782	9.781504	-0.061256	4.816033
300.389304	8000.236724	9.786509	-0.061251	4.816008
300.679263	8000.310458	9.791514	-0.061306	4.816028
300.587555	8000.252133	9.796519	-0.061289	4.816011
300.635090	8000.216668	9.801523	-0.061297	4.816000
300.671413	8000.263311	9.806528	-0.061304	4.816014
300.655571	8000.183926	9.811533	-0.061302	4.815991
300.731526	8000.292226	9.816538	-0.061316	4.816022
300.715535	8000.263081	9.821543	-0.061313	4.816014
300.740743	8000.221863	9.826547	-0.061318	4.816001
300.766913	8000.280078	9.831552	-0.061323	4.816018
300.778094	8000.249293	9.836557	-0.061325	4.816009
300.921262	8000.263684	9.841562	-0.061352	4.816013
300.704675	8000.270419	9.846567	-0.061311	4.816016
300.478912	8000.241710	9.851571	-0.061270	4.816009
300.826051	8000.333596	9.856576	-0.061334	4.816034
300.771872	8000.279164	9.861581	-0.061324	4.816018
300.650649	8000.322923	9.866586	-0.061302	4.816031
300.627681	8000.303271	9.871591	-0.061298	4.816026
300.809942	8000.218961	9.876595	-0.061332	4.816000
300.814361	8000.301365	9.881600	-0.061333	4.816024
300.876267	8000.216989	9.886605	-0.061344	4.815999
300.851402	8000.282823	9.891610	-0.061340	4.816019
300.891408	8000.242944	9.896615	-0.061347	4.816007
300.591830	8000.255643	9.901619	-0.061292	4.816012
300.856842	8000.278678	9.906624	-0.061341	4.816017
300.873675	8000.227685	9.911629	-0.061344	4.816002
300.683719	8000.305462	9.916634	-0.061309	4.816026
300.899088	8000.275208	9.921639	-0.061349	4.816016
300.946111	8000.161697	9.926643	-0.061358	4.815983
300.920310	8000.225375	9.931648	-0.061353	4.816001
300.628367	8000.190109	9.936653	-0.061299	4.815993
300.995119	8000.306941	9.941658	-0.061368	4.816025
300.706009	8000.233243	9.946663	-0.061314	4.816005
300.722632	8000.219661	9.951667	-0.061317	4.816001
300.807378	8000.241534	9.956672	-0.061333	4.816007
300.807007	8000.150673	9.961677	-0.061333	4.815980
300.814626	8000.254516	9.966682	-0.061335	4.816010
300.670065	8000.244397	9.971687	-0.061308	4.816008
300.867744	8000.238406	9.976691	-0.061345	4.816005
300.914295	8000.244614	9.981696	-0.061353	4.816007
300.849540	8000.195334	9.986701	-0.061341	4.815993
300.955838	8000.257155	9.991706	-0.061361	4.816010
300.859235	8000.190188	9.996711	-0.061343	4.815991
300.736436	8000.197572	10.001715	-0.061321	4.815994
300.750758	8000.220293	10.006720	-0.061323	4.816001
300.810441	8000.232087	10.011725	-0.061335	4.816004
300.866179	8000.285499	10.016730	-0.061345	4.816019
300.969237	8000.277775	10.021735	-0.061365	4.816016
300.860191	8000.195615	10.026739	-0.061344	4.815993
301.032197	8000.278950	10.031744	-0.061376	4.816016
300.894896	8000.245445	10.036749	-0.061351	4.816007
301.025228	8000.282050	10.041754	-0.061375	4.816017
300.982171	8000.208581	10.046759	-0.061367	4.815996
300.986486	8000.141323	10.051763	-0.061368	4.815976
301.201968	8000.191246	10.056768	-0.061409	4.815990
301.075168	8000.181452	10.061773	-0.061385	4.815988
300.985957	8000.240763	10.066778	-0.061369	4.816005
300.832522	8000.250792	10.071783	-0.061340	4.816009
301.123675	8000.170613	10.076787	-0.061394	4.815984
301.250979	8000.263820	10.081792	-0.061418	4.816011
301.218805	8000.239724	10.086797	-0.061412	4.816004
301.163590	8000.286829	10.091802	-0.061402	4.816018
301.298416	8000.236927	10.096807	-0.061427	4.816003
301.052032	8000.201425	10.101811	-0.061382	4.815994
301.110480	8000.236714	10.106816	-0.061393	4.816004
301.336067	8000.251546	10.111821	-0.061435	4.816007
301.352387	8000.332031	10.116826	-0.061438	4.816030
301.180124	8000.249781	10.121831	-0.061406	4.816007
301.316882	8000.187086	10.126835	-0.061432	4.815988
301.403222	8000.269922	10.131840	-0.061448	4.816012
301.199097	8000.181744	10.136845	-0.061410	4.815987
301.260688	8000.247023	10.141850	-0.061421	4.816006
301.264715	8000.172277	10.146855	-0.061422	4.815984
301.154591	8000.203410	10.151859	-0.061402	4.815994
301.291831	8000.302144	10.156864	-0.061428	4.816022
301.213940	8000.173517	10.161869	-0.061413	4.815985
301.202114	8000.196829	10.166874	-0.061411	4.815991
301.049439	8000.259254	10.171879	-0.061383	4.816010
301.258563	8000.262025	10.176883	-0.061422	4.816010
301.297539	8000.306579	10.181888	-0.061429	4.816023
301.265774	8000.255764	10.186893	-0.061423	4.816008
301.284788	8000.270020	10.191898	-0.061427	4.816012
301.363052	8000.227634	10.196903	-0.061442	4.816000
301.375659	8000.268498	10.201907	-0.061444	4.816011
301.395838	8000.272086	10.206912	-0.061448	4.816012
301.397200	8000.225085	10.211917	-0.061448	4.815999
301.501073	8000.268689	10.216922	-0.061468	4.816011
301.347343	8000.258402	10.221927	-0.061439	4.816009
301.165709	8000.241189	10.226931	-0.061406	4.816005
301.268725	8000.282640	10.231936	-0.061425	4.816016
301.319041	8000.208741	10.236941	-0.061434	4.815994
301.193083	8000.250275	10.241946	-0.061411	4.816007
301.316151	8000.288885	10.246951	-0.061434	4.816018
301.334005	8000.252877	10.251955	-0.061437	4.816007
301.248765	8000.330433	10.256960	-0.061422	4.816030
301.246650	8000.273747	10.261965	-0.061421	4.816014
301.292370	8000.330184	10.266970	-0.061430	4.816030
301.138835	8000.256829	10.271975	-0.061402	4.816009
301.248632	8000.232125	10.276979	-0.061422	4.816001
301.376609	8000.252652	10.281984	-0.061446	4.816007
301.308333	8000.258895	10.286989	-0.061433	4.816009
301.422284	8000.215025	10.291994	-0.061455	4.815995
301.553720	8000.287998	10.296999	-0.061479	4.816016
301.411224	8000.234086	10.302003	-0.061453	4.816001
301.428416	8000.282517	10.307008	-0.061456	4.816015
301.435276	8000.229203	10.312013	-0.061458	4.816000
301.495696	8000.254908	10.317018	-0.061469	4.816007
301.594681	8000.250317	10.322023	-0.061488	4.816005
301.656131	8000.273902	10.327027	-0.061499	4.816011
301.601042	8000.292147	10.332032	-0.061489	4.816017
301.557132	8000.200487	10.337037	-0.061481	4.815990
301.590050	8000.291967	10.342042	-0.061487	4.816017
301.528993	8000.234201	10.347047	-0.061476	4.816000
301.489323	8000.188587	10.352051	-0.061469	4.815987
301.518633	8000.285346	10.357056	-0.061474	4.816015
301.463788	8000.286490	10.362061	-0.061464	4.816016
301.610683	8000.306295	10.367066	-0.061492	4.816021
301.571511	8000.290622	10.372071	-0.061484	4.816017
301.637605	8000.312155	10.377075	-0.061497	4.816023
301.659722	8000.345710	10.382080	-0.061501	4.816032
301.456327	8000.243646	10.387085	-0.061463	4.816004
301.576640	8000.320692	10.392090	-0.061486	4.816025
301.537745	8000.278298	10.397095	-0.061479	4.816013
301.777780	8000.236737	10.402099	-0.061523	4.816000
301.694329	8000.289740	10.407104	-0.061508	4.816016
301.731909	8000.254092	10.412109	-0.061515	4.816005
301.691004	8000.269389	10.417114	-0.061508	4.816010
301.709761	8000.275088	10.422119	-0.061511	4.816011
301.508330	8000.188026	10.427123	-0.061474	4.815987
301.834119	8000.301975	10.432128	-0.061535	4.816019
301.757890	8000.252483	10.437133	-0.061520	4.816005
301.682391	8000.271422	10.442138	-0.061506	4.816010
301.771953	8000.294454	10.447143	-0.061523	4.816017
301.726059	8000.223069	10.452147	-0.061515	4.815996
301.824731	8000.278338	10.457152	-0.061533	4.816012
301.774271	8000.223973	10.462157	-0.061524	4.815996
302.022701	8000.336506	10.467162	-0.061570	4.816028
301.930814	8000.299555	10.472167	-0.061553	4.816017
301.726820	8000.226343	10.477171	-0.061515	4.815997
301.950573	8000.256109	10.482176	-0.061557	4.816005
301.774916	8000.230452	10.487181	-0.061525	4.815998
301.620655	8000.297124	10.492186	-0.061496	4.816018
301.770930	8000.249643	10.497191	-0.061524	4.816004
301.834617	8000.195231	10.502195	-0.061536	4.815987
301.585629	8000.207786	10.507200	-0.061490	4.815992
301.630061	8000.205404	10.512205	-0.061498	4.815991
301.815110	8000.267600	10.517210	-0.061533	4.816009
301.758289	8000.264432	10.522215	-0.061522	4.816008
301.743342	8000.198958	10.527219	-0.061520	4.815989
301.812298	8000.300720	10.532224	-0.061533	4.816018
301.855163	8000.274790	10.537229	-0.061541	4.816010
301.768145	8000.291380	10.542234	-0.061525	4.816016
301.640772	8000.280506	10.547239	-0.061501	4.816013
301.839578	8000.259570	10.552243	-0.061538	4.816006
301.907188	8000.319616	10.557248	-0.061551	4.816023
301.853708	8000.297267	10.562253	-0.061541	4.816017
301.968532	8000.296173	10.567258	-0.061562	4.816016
301.825018	8000.316005	10.572263	-0.061536	4.816023
301.704262	8000.271043	10.577267	-0.061513	4.816010
301.826574	8000.338505	10.582272	-0.061536	4.816029
301.778424	8000.290596	10.587277	-0.061528	4.816015
301.747923	8000.349914	10.592282	-0.061522	4.816033
301.665576	8000.334519	10.597287	-0.061507	4.816029
301.893864	8000.266017	10.602291	-0.061549	4.816008
301.963779	8000.326105	10.607296	-0.061562	4.816025
301.747311	8000.306115	10.612301	-0.061522	4.816020
302.103888	8000.246377	10.617306	-0.061589	4.816001
301.984383	8000.315824	10.622311	-0.061567	4.816022
301.882993	8000.284045	10.627315	-0.061548	4.816013
301.986496	8000.321229	10.632320	-0.061567	4.816023
301.896989	8000.285392	10.637325	-0.061551	4.816013
302.037679	8000.274082	10.642330	-0.061577	4.816009
301.648793	8000.278729	10.647335	-0.061505	4.816013
301.678492	8000.234385	10.652339	-0.061510	4.816000
301.987324	8000.260363	10.657344	-0.061568	4.816005
301.849073	8000.258911	10.662349	-0.061542	4.816006
301.993715	8000.316091	10.667354	-0.061569	4.816022
302.052264	8000.277620	10.672359	-0.061580	4.816010
302.021337	8000.174438	10.677363	-0.061575	4.815980
302.084231	8000.316713	10.682368	-0.061587	4.816021
302.023233	8000.286742	10.687373	-0.061575	4.816013
302.024269	8000.302807	10.692378	-0.061576	4.816018
301.826020	8000.317360	10.697383	-0.061539	4.816023
301.900987	8000.258878	10.702387	-0.061553	4.816005
301.995257	8000.276651	10.707392	-0.061570	4.816010
301.853079	8000.154327	10.712397	-0.061544	4.815975
301.920655	8000.179094	10.717402	-0.061557	4.815982
301.980623	8000.281760	10.722407	-0.061568	4.816012
302.080925	8000.282539	10.727411	-0.061587	4.816011
302.087538	8000.307259	10.732416	-0.061588	4.816019
302.168672	8000.290582	10.737421	-0.061603	4.816013
302.308790	8000.248260	10.742426	-0.061630	4.816000
302.206600	8000.295575	10.747431	-0.061611	4.816015
302.103777	8000.246664	10.752435	-0.061592	4.816001
302.043031	8000.309704	10.757440	-0.061580	4.816020
301.917836	8000.275351	10.762445	-0.061557	4.816010
302.075300	8000.329559	10.767450	-0.061587	4.816025
302.154844	8000.318199	10.772455	-0.061602	4.816021
302.028156	8000.321234	10.777459	-0.061578	4.816023
301.968817	8000.274189	10.782464	-0.061567	4.816010
302.027785	8000.243209	10.787469	-0.061578	4.816000
302.113335	8000.289686	10.792474	-0.061594	4.816013
302.129850	8000.254721	10.797479	-0.061597	4.816003
302.278455	8000.272421	10.802483	-0.061625	4.816007
302.384009	8000.337439	10.807488	-0.061645	4.816026
302.213955	8000.283020	10.812493	-0.061614	4.816011
302.122599	8000.318774	10.817498	-0.061597	4.816022
302.355999	8000.249296	10.822503	-0.061640	4.816000
302.298804	8000.195877	10.827507	-0.061630	4.815985
302.256084	8000.310561	10.832512	-0.061622	4.816019
302.150242	8000.331082	10.837517	-0.061602	4.816025
302.094166	8000.339687	10.842522	-0.061592	4.816028
302.226050	8000.291869	10.847527	-0.061617	4.816013
302.149784	8000.230617	10.852531	-0.061602	4.815996
302.364723	8000.338262	10.857536	-0.061643	4.816026
302.164498	8000.228769	10.862541	-0.061605	4.815995
302.264643	8000.237029	10.867546	-0.061624	4.815997
302.349475	8000.294184	10.872551	-0.061640	4.816013
302.178171	8000.267537	10.877555	-0.061608	4.816006
302.134845	8000.360830	10.882560	-0.061600	4.816034
302.020391	8000.296739	10.887565	-0.061579	4.816016
302.166156	8000.212829	10.892570	-0.061606	4.815990
302.342822	8000.282356	10.897575	-0.061639	4.816010
302.075500	8000.278538	10.902579	-0.061590	4.816010
302.142286	8000.334293	10.907584	-0.061602	4.816026
302.131638	8000.290279	10.912589	-0.061600	4.816013
302.278769	8000.302606	10.917594	-0.061628	4.816016
302.310830	8000.302135	10.922599	-0.061634	4.816016
302.308812	8000.285004	10.927603	-0.061634	4.816011
302.382735	8000.322716	10.932608	-0.061648	4.816021
302.099257	8000.256599	10.937613	-0.061595	4.816004
302.119098	8000.236661	10.942618	-0.061599	4.815998
302.110359	8000.298516	10.947623	-0.061597	4.816016
302.237779	8000.283756	10.952627	-0.061621	4.816011
302.489375	8000.345036	10.957632	-0.061668	4.816027
302.293955	8000.284807	10.962637	-0.061632	4.816011
302.342647	8000.300676	10.967642	-0.061641	4.816015
302.284643	8000.335972	10.972647	-0.061630	4.816026
302.179647	8000.294504	10.977651	-0.061611	4.816014
302.196195	8000.354684	10.982656	-0.061614	4.816032
302.160776	8000.307008	10.987661	-0.061607	4.816018
302.303780	8000.286120	10.992666	-0.061634	4.816011
302.189902	8000.304356	10.997671	-0.061613	4.816017
302.178712	8000.265677	11.002675	-0.061611	4.816006
302.381844	8000.326068	11.007680	-0.061649	4.816022
302.294676	8000.318067	11.012685	-0.061633	4.816020
302.410431	8000.312715	11.017690	-0.061655	4.816018
302.536893	8000.339631	11.022695	-0.061678	4.816025
302.439572	8000.283338	11.027699	-0.061660	4.816010
302.350058	8000.316987	11.032704	-0.061644	4.816020
302.389872	8000.286725	11.037709	-0.061651	4.816011
302.552613	8000.330341	11.042714	-0.061682	4.816023
302.486803	8000.328077	11.047719	-0.061669	4.816022
302.212426	8000.236468	11.052723	-0.061618	4.815997
302.485937	8000.248973	11.057728	-0.061669	4.815999
302.399926	8000.247408	11.062733	-0.061654	4.815999
302.358568	8000.279801	11.067738	-0.061646	4.816009
302.376374	8000.272655	11.072743	-0.061649	4.816007
302.515990	8000.276292	11.077747	-0.061676	4.816007
302.552160	8000.329349	11.082752	-0.061682	4.816022
302.258128	8000.284418	11.087757	-0.061628	4.816011
302.484287	8000.292848	11.092762	-0.061670	4.816012
302.358090	8000.275580	11.097767	-0.061647	4.816008
302.378650	8000.259932	11.102771	-0.061650	4.816003
302.456356	8000.339407	11.107776	-0.061665	4.816026
302.569735	8000.286973	11.112781	-0.061686	4.816010
302.650790	8000.322679	11.117786	-0.061702	4.816020
302.416685	8000.297019	11.122791	-0.061658	4.816014
302.308949	8000.297194	11.127795	-0.061638	4.816014
302.367225	8000.381658	11.132800	-0.061649	4.816039
302.248064	8000.292893	11.137805	-0.061627	4.816013
302.461468	8000.292537	11.142810	-0.061667	4.816012
302.641836	8000.307612	11.147815	-0.061700	4.816015
302.488798	8000.196846	11.152819	-0.061672	4.815984
302.412053	8000.354738	11.157824	-0.061658	4.816030
302.539042	8000.283311	11.162829	-0.061682	4.816009
302.469310	8000.248904	11.167834	-0.061669	4.815999
302.584680	8000.353657	11.172839	-0.061690	4.816029
302.614569	8000.299694	11.177843	-0.061696	4.816013
302.686497	8000.323472	11.182848	-0.061710	4.816020
302.500538	8000.262347	11.187853	-0.061675	4.816003
302.419448	8000.261941	11.192858	-0.061660	4.816003
302.727898	8000.314642	11.197863	-0.061718	4.816017
302.340243	8000.296859	11.202867	-0.061646	4.816014
302.558176	8000.394939	11.207872	-0.061686	4.816041
302.597654	8000.326185	11.212877	-0.061694	4.816021
302.498017	8000.340406	11.217882	-0.061675	4.816026
302.423105	8000.356148	11.222887	-0.061661	4.816031
302.474790	8000.280135	11.227891	-0.061671	4.816008
302.579382	8000.365448	11.232896	-0.061691	4.816033
302.522022	8000.299195	11.237901	-0.061680	4.816014
302.605162	8000.330663	11.242906	-0.061696	4.816022
302.827002	8000.330462	11.247911	-0.061737	4.816021
302.701823	8000.291831	11.252915	-0.061714	4.816010
302.538542	8000.293127	11.257920	-0.061684	4.816012
302.558227	8000.310603	11.262925	-0.061687	4.816017
302.724845	8000.354290	11.267930	-0.061719	4.816029
302.675280	8000.351255	11.272935	-0.061709	4.816028
302.575414	8000.325916	11.277939	-0.061691	4.816021
302.638095	8000.342042	11.282944	-0.061703	4.816025
302.604705	8000.283713	11.287949	-0.061697	4.816009
302.561143	8000.302168	11.292954	-0.061689	4.816014
302.633505	8000.336645	11.297959	-0.061702	4.816024
302.556494	8000.278585	11.302963	-0.061688	4.816007
302.722629	8000.295538	11.307968	-0.061719	4.816011
302.731595	8000.351303	11.312973	-0.061721	4.816028
302.580739	8000.320754	11.317978	-0.061693	4.816020
302.549538	8000.310572	11.322983	-0.061687	4.816017
302.733248	8000.284015	11.327987	-0.061721	4.816008
302.712398	8000.280437	11.332992	-0.061718	4.816007
302.656842	8000.245220	11.337997	-0.061707	4.815997
302.468005	8000.287740	11.343002	-0.061672	4.816010
302.650932	8000.349900	11.348007	-0.061707	4.816028
302.674202	8000.256261	11.353011	-0.061711	4.816000
302.686592	8000.314227	11.358016	-0.061713	4.816017
302.642315	8000.304874	11.363021	-0.061705	4.816015
302.657367	8000.261330	11.368026	-0.061708	4.816002
302.605628	8000.318121	11.373031	-0.061699	4.816019
302.710216	8000.262319	11.378035	-0.061718	4.816002
302.712191	8000.346821	11.383040	-0.061719	4.816026
302.525689	8000.298515	11.388045	-0.061684	4.816013
302.654505	8000.251709	11.393050	-0.061708	4.815999
302.694788	8000.327292	11.398055	-0.061716	4.816021
302.500060	8000.308768	11.403059	-0.061680	4.816016
302.491781	8000.358872	11.408064	-0.061678	4.816031
302.583027	8000.304964	11.413069	-0.061695	4.816015
302.803434	8000.250215	11.418074	-0.061736	4.815998
302.712999	8000.284917	11.423079	-0.061720	4.816008
302.476847	8000.245322	11.428083	-0.061676	4.815998
302.743506	8000.314362	11.433088	-0.061726	4.816017
302.658142	8000.314946	11.438093	-0.061710	4.816017
302.665828	8000.317236	11.443098	-0.061711	4.816018
302.776606	8000.356694	11.448103	-0.061732	4.816029
302.848111	8000.276766	11.453107	-0.061746	4.816005
302.874693	8000.299714	11.458112	-0.061751	4.816012
302.838080	8000.256292	11.463117	-0.061744	4.815999
302.772143	8000.215540	11.468122	-0.061732	4.815988
302.751488	8000.298558	11.473127	-0.061728	4.816012
302.767733	8000.303142	11.478131	-0.061731	4.816013
302.605740	8000.318359	11.483136	-0.061701	4.816019
302.584992	8000.308368	11.488141	-0.061697	4.816016
302.564259	8000.256684	11.493146	-0.061694	4.816001
302.769270	8000.334216	11.498151	-0.061732	4.816022
302.762417	8000.246439	11.503155	-0.061731	4.815997
302.768168	8000.285041	11.508160	-0.061732	4.816008
302.520179	8000.281577	11.513165	-0.061686	4.816008
302.862951	8000.273970	11.518170	-0.061750	4.816004
302.976528	8000.329515	11.523175	-0.061771	4.816020
302.882271	8000.265793	11.528179	-0.061753	4.816002
302.673244	8000.343222	11.533184	-0.061715	4.816025
302.550793	8000.266155	11.538189	-0.061692	4.816004
302.595551	8000.268055	11.543194	-0.061700	4.816004
302.878512	8000.305322	11.548199	-0.061753	4.816013
302.798163	8000.205508	11.553203	-0.061738	4.815985
302.897796	8000.285385	11.558208	-0.061757	4.816007
302.610253	8000.280127	11.563213	-0.061704	4.816007
302.739458	8000.309231	11.568218	-0.061728	4.816015
302.698322	8000.323455	11.573223	-0.061720	4.816020
302.745778	8000.265537	11.578227	-0.061729	4.816002
302.849224	8000.318758	11.583232	-0.061749	4.816017
302.776876	8000.238333	11.588237	-0.061735	4.815994
302.860005	8000.228108	11.593242	-0.061751	4.815991
302.915429	8000.259067	11.598247	-0.061761	4.816000
302.793846	8000.285715	11.603251	-0.061739	4.816008
302.713579	8000.364434	11.608256	-0.061724	4.816031
302.665901	8000.271632	11.613261	-0.061715	4.816005
302.860381	8000.251687	11.618266	-0.061751	4.815998
302.930524	8000.343853	11.623271	-0.061765	4.816024
302.773800	8000.335646	11.628275	-0.061736	4.816023
302.913207	8000.286897	11.633280	-0.061762	4.816008
302.895153	8000.270541	11.638285	-0.061758	4.816003
302.744305	8000.275271	11.643290	-0.061730	4.816005
302.974483	8000.362886	11.648295	-0.061773	4.816030
302.900058	8000.284561	11.653299	-0.061760	4.816007
302.965807	8000.344575	11.658304	-0.061772	4.816024
302.850380	8000.274050	11.663309	-0.061750	4.816004
303.004985	8000.291861	11.668314	-0.061779	4.816009
302.861539	8000.299934	11.673319	-0.061753	4.816012
302.718295	8000.265248	11.678323	-0.061726	4.816002
302.917573	8000.319156	11.683328	-0.061763	4.816017
302.957466	8000.303862	11.688333	-0.061771	4.816012
302.966941	8000.304046	11.693338	-0.061773	4.816012
303.033798	8000.332009	11.698343	-0.061785	4.816020
303.130216	8000.274988	11.703347	-0.061803	4.816003
302.843527	8000.265469	11.708352	-0.061750	4.816002
302.918666	8000.210196	11.713357	-0.061764	4.815985
302.964936	8000.176845	11.718362	-0.061773	4.815975
303.106323	8000.266040	11.723367	-0.061799	4.816000
302.907651	8000.259203	11.728371	-0.061763	4.816000
303.012474	8000.315657	11.733376	-0.061782	4.816015
302.915030	8000.309606	11.738381	-0.061764	4.816014
302.931990	8000.297098	11.743386	-0.061767	4.816010
302.782376	8000.345682	11.748391	-0.061740	4.816025
302.697098	8000.276780	11.753395	-0.061724	4.816006
302.908475	8000.317012	11.758400	-0.061763	4.816016
302.735715	8000.287130	11.763405	-0.061731	4.816009
303.015525	8000.206744	11.768410	-0.061783	4.815984
303.100824	8000.309878	11.773415	-0.061800	4.816013
303.015060	8000.342527	11.778419	-0.061784	4.816023
302.999936	8000.364711	11.783424	-0.061781	4.816030
302.903659	8000.369372	11.788429	-0.061763	4.816032
302.850663	8000.328856	11.793434	-0.061753	4.816020
302.899710	8000.303039	11.798439	-0.061763	4.816012
302.985900	8000.271488	11.803443	-0.061779	4.816003
302.874556	8000.359260	11.808448	-0.061758	4.816029
302.885484	8000.318846	11.813453	-0.061760	4.816017
302.865271	8000.298174	11.818458	-0.061757	4.816011
303.005486	8000.325343	11.823463	-0.061783	4.816018
303.068743	8000.289096	11.828467	-0.061795	4.816007
303.053818	8000.329457	11.833472	-0.061792	4.816019
302.976589	8000.318431	11.838477	-0.061778	4.816016
303.022059	8000.236958	11.843482	-0.061786	4.815992
303.072962	8000.264628	11.848487	-0.061796	4.816000
302.949575	8000.207855	11.853491	-0.061773	4.815984
303.081018	8000.308628	11.858496	-0.061798	4.816013
303.117420	8000.355276	11.863501	-0.061805	4.816026
303.140985	8000.252019	11.868506	-0.061809	4.815996
303.028392	8000.345113	11.873511	-0.061788	4.816024
302.905712	8000.303320	11.878515	-0.061765	4.816012
302.956223	8000.405818	11.883520	-0.061775	4.816042
302.886071	8000.356435	11.888525	-0.061762	4.816028
302.810156	8000.291980	11.893530	-0.061748	4.816010
302.853710	8000.346241	11.898535	-0.061756	4.816025
302.729631	8000.285180	11.903539	-0.061733	4.816008
303.017846	8000.378136	11.908544	-0.061787	4.816034
303.063667	8000.375779	11.913549	-0.061796	4.816033
302.963599	8000.280947	11.918554	-0.061777	4.816005
303.094548	8000.358192	11.923559	-0.061802	4.816027
302.858100	8000.260862	11.928563	-0.061758	4.816000
302.957116	8000.337521	11.933568	-0.061776	4.816022
302.942220	8000.316946	11.938573	-0.061774	4.816016
303.000141	8000.315881	11.943578	-0.061785	4.816015
303.130476	8000.351421	11.948583	-0.061809	4.816025
303.125843	8000.288272	11.953587	-0.061808	4.816007
303.270870	8000.310184	11.958592	-0.061835	4.816012
302.805722	8000.299532	11.963597	-0.061749	4.816012
302.835994	8000.293683	11.968602	-0.061754	4.816010
303.117525	8000.282817	11.973607	-0.061807	4.816005
303.043957	8000.206645	11.978611	-0.061793	4.815983
303.191776	8000.284199	11.983616	-0.061821	4.816005
302.938054	8000.324461	11.988621	-0.061774	4.816018
302.820531	8000.291315	11.993626	-0.061752	4.816009
303.094361	8000.317725	11.998631	-0.061803	4.816015
303.099847	8000.305008	12.003635	-0.061804	4.816012
303.243737	8000.285205	12.008640	-0.061831	4.816005
303.165195	8000.327608	12.013645	-0.061817	4.816018
303.069614	8000.305555	12.018650	-0.061799	4.816012
303.058278	8000.353465	12.023655	-0.061797	4.816026
302.926516	8000.309368	12.028659	-0.061773	4.816014
303.117395	8000.329982	12.033664	-0.061808	4.816019
303.111287	8000.298878	12.038669	-0.061807	4.816010
303.254912	8000.325040	12.043674	-0.061834	4.816017
303.203005	8000.340136	12.048679	-0.061825	4.816021
303.117255	8000.316124	12.053683	-0.061809	4.816015
303.062503	8000.335444	12.058688	-0.061799	4.816021
302.953368	8000.323833	12.063693	-0.061778	4.816018
302.958000	8000.307893	12.068698	-0.061779	4.816013
303.000143	8000.331126	12.073703	-0.061787	4.816020
303.115389	8000.261621	12.078707	-0.061809	4.815999
302.971655	8000.307106	12.083712	-0.061782	4.816013
302.982369	8000.320142	12.088717	-0.061784	4.816017
303.000968	8000.318355	12.093722	-0.061788	4.816016
303.126434	8000.352737	12.098727	-0.061811	4.816025
303.062387	8000.303466	12.103731	-0.061800	4.816011
303.151507	8000.310455	12.108736	-0.061816	4.816013
303.247158	8000.352844	12.113741	-0.061834	4.816025
303.229146	8000.332212	12.118746	-0.061831	4.816019
303.308861	8000.339029	12.123751	-0.061846	4.816020
303.212251	8000.289161	12.128755	-0.061828	4.816006
303.122254	8000.355943	12.133760	-0.061811	4.816026
303.107146	8000.321466	12.138765	-0.061809	4.816016
303.050313	8000.276604	12.143770	-0.061798	4.816004
302.993754	8000.333308	12.148775	-0.061788	4.816020
303.041435	8000.301051	12.153779	-0.061797	4.816011
303.103813	8000.313965	12.158784	-0.061808	4.816014
303.019628	8000.314571	12.163789	-0.061793	4.816015
303.074640	8000.276034	12.168794	-0.061803	4.816003
303.238990	8000.264090	12.173799	-0.061834	4.815999
303.228720	8000.254291	12.178803	-0.061832	4.815996
303.270350	8000.319209	12.183808	-0.061840	4.816015
303.241080	8000.326166	12.188813	-0.061835	4.816017
303.158167	8000.270135	12.193818	-0.061819	4.816001
303.428700	8000.302900	12.198823	-0.061870	4.816009
303.209707	8000.308518	12.203827	-0.061829	4.816012
303.403382	8000.256487	12.208832	-0.061865	4.815996
303.440034	8000.283896	12.213837	-0.061872	4.816004
303.386188	8000.269022	12.218842	-0.061862	4.816000
303.399593	8000.351597	12.223847	-0.061865	4.816024
303.324288	8000.285014	12.228851	-0.061851	4.816005
303.255263	8000.317970	12.233856	-0.061838	4.816015
303.297960	8000.332661	12.238861	-0.061846	4.816019
303.434114	8000.329822	12.243866	-0.061872	4.816017
303.425806	8000.380996	12.248871	-0.061870	4.816032
303.244105	8000.315670	12.253875	-0.061837	4.816014
303.440538	8000.306453	12.258880	-0.061873	4.816010
303.400682	8000.351703	12.263885	-0.061866	4.816024
303.250410	8000.281608	12.268890	-0.061838	4.816004
303.366782	8000.301926	12.273895	-0.061860	4.816009
303.400867	8000.314321	12.278899	-0.061866	4.816013
303.358376	8000.371283	12.283904	-0.061859	4.816030
303.240427	8000.332783	12.288909	-0.061837	4.816019
303.398253	8000.283302	12.293914	-0.061866	4.816004
303.422635	8000.373562	12.298919	-0.061871	4.816030
303.138348	8000.291389	12.303923	-0.061818	4.816007
303.385767	8000.303418	12.308928	-0.061864	4.816010
303.199647	8000.303224	12.313933	-0.061830	4.816010
303.174086	8000.283523	12.318938	-0.061825	4.816005
303.163596	8000.291894	12.323943	-0.061823	4.816007
303.360684	8000.275205	12.328947	-0.061860	4.816001
303.415880	8000.244155	12.333952	-0.061870	4.815992
303.381636	8000.302337	12.338957	-0.061864	4.816009
303.494053	8000.262714	12.343962	-0.061885	4.815997
303.413580	8000.325395	12.348967	-0.061870	4.816016
303.482080	8000.310625	12.353971	-0.061883	4.816011
303.482155	8000.361952	12.358976	-0.061883	4.816026
303.526670	8000.343536	12.363981	-0.061892	4.816020
303.450501	8000.321838	12.368986	-0.061878	4.816015
303.454246	8000.334746	12.373991	-0.061878	4.816018
303.596460	8000.262528	12.378995	-0.061905	4.815996
303.753400	8000.301764	12.384000	-0.061934	4.816007
303.383293	8000.315303	12.389005	-0.061866	4.816013
303.276189	8000.194685	12.394010	-0.061846	4.815978
303.500533	8000.324957	12.399015	-0.061888	4.816015
303.396483	8000.312370	12.404019	-0.061868	4.816012
303.388901	8000.358212	12.409024	-0.061867	4.816025
303.594162	8000.319222	12.414029	-0.061905	4.816013
303.590928	8000.320243	12.419034	-0.061905	4.816013
303.540855	8000.357822	12.424039	-0.061896	4.816025
303.627315	8000.309171	12.429043	-0.061912	4.816010
303.663226	8000.376123	12.434048	-0.061919	4.816029
303.420480	8000.341750	12.439053	-0.061874	4.816020
303.490222	8000.323796	12.444058	-0.061887	4.816015
303.699574	8000.381098	12.449063	-0.061926	4.816030
303.503368	8000.350785	12.454067	-0.061889	4.816023
303.646802	8000.311731	12.459072	-0.061916	4.816010
303.662074	8000.324851	12.464077	-0.061919	4.816014
303.596043	8000.280888	12.469082	-0.061907	4.816002
303.550917	8000.312144	12.474087	-0.061899	4.816011
303.365137	8000.222154	12.479091	-0.061864	4.815986
303.521452	8000.282760	12.484096	-0.061893	4.816003
303.519528	8000.283804	12.489101	-0.061893	4.816003
303.347771	8000.319154	12.494106	-0.061861	4.816014
303.458964	8000.389623	12.499111	-0.061882	4.816034
303.350902	8000.348097	12.504115	-0.061862	4.816023
303.388618	8000.288931	12.509120	-0.061869	4.816005
303.603299	8000.328157	12.514125	-0.061909	4.816015
303.663880	8000.300413	12.519130	-0.061921	4.816007
303.522511	8000.351286	12.524135	-0.061894	4.816023
303.667584	8000.263084	12.529139	-0.061921	4.815996
303.697455	8000.326718	12.534144	-0.061927	4.816015
303.434343	8000.317630	12.539149	-0.061878	4.816013
303.498475	8000.315609	12.544154	-0.061890	4.816012
303.713089	8000.374077	12.549159	-0.061930	4.816028
303.723661	8000.270580	12.554163	-0.061932	4.815998
303.373108	8000.251337	12.559168	-0.061867	4.815994
303.548247	8000.278077	12.564173	-0.061900	4.816001
303.831649	8000.189204	12.569178	-0.061953	4.815974
303.671494	8000.338088	12.574183	-0.061923	4.816018
303.497514	8000.334909	12.579187	-0.061891	4.816018
303.550760	8000.359416	12.584192	-0.061901	4.816025
303.497543	8000.359520	12.589197	-0.061891	4.816025
303.436934	8000.263272	12.594202	-0.061880	4.815997
303.715352	8000.303666	12.599207	-0.061932	4.816008
303.591509	8000.272541	12.604211	-0.061909	4.815999
303.645679	8000.279959	12.609216	-0.061919	4.816001
303.498461	8000.340347	12.614221	-0.061892	4.816020
303.476994	8000.266198	12.619226	-0.061888	4.815998
303.485406	8000.345474	12.624231	-0.061890	4.816021
303.440834	8000.263419	12.629235	-0.061881	4.815997
303.450175	8000.317054	12.634240	-0.061883	4.816013
303.403286	8000.327965	12.639245	-0.061875	4.816016
303.541611	8000.296301	12.644250	-0.061901	4.816006
303.767572	8000.316490	12.649255	-0.061943	4.816011
303.698723	8000.291719	12.654259	-0.061930	4.816004
303.638728	8000.312011	12.659264	-0.061919	4.816010
303.710346	8000.334717	12.664269	-0.061932	4.816017
303.633559	8000.249932	12.669274	-0.061918	4.815992
303.694136	8000.350477	12.674279	-0.061930	4.816021
303.549429	8000.359595	12.679283	-0.061903	4.816025
303.621032	8000.319224	12.684288	-0.061916	4.816013
303.503977	8000.324573	12.689293	-0.061895	4.816015
303.368065	8000.291089	12.694298	-0.061869	4.816006
303.471893	8000.287657	12.699303	-0.061889	4.816004
303.487430	8000.254812	12.704307	-0.061892	4.815995
303.443891	8000.259370	12.709312	-0.061884	4.815996
303.401385	8000.290673	12.714317	-0.061876	4.816005
303.451888	8000.268090	12.719322	-0.061885	4.815999
303.689596	8000.322705	12.724327	-0.061930	4.816013
303.632071	8000.296003	12.729331	-0.061919	4.816006
303.675280	8000.231592	12.734336	-0.061927	4.815987
303.657978	8000.247322	12.739341	-0.061924	4.815991
303.769097	8000.294271	12.744346	-0.061945	4.816005
303.706445	8000.340173	12.749351	-0.061934	4.816018
303.608566	8000.323422	12.754355	-0.061915	4.816014
303.723655	8000.328750	12.759360	-0.061937	4.816015
303.562302	8000.363220	12.764365	-0.061907	4.816026
303.664341	8000.354411	12.769370	-0.061926	4.816023
303.761833	8000.387212	12.774375	-0.061944	4.816032
303.549730	8000.340571	12.779379	-0.061905	4.816019
303.597785	8000.291216	12.784384	-0.061914	4.816005
303.830546	8000.314737	12.789389	-0.061958	4.816010
303.656861	8000.294459	12.794394	-0.061925	4.816005
303.680292	8000.341938	12.799399	-0.061930	4.816019
303.720589	8000.286027	12.804403	-0.061937	4.816002
303.745820	8000.313227	12.809408	-0.061942	4.816010
303.664239	8000.363058	12.814413	-0.061927	4.816025
303.815697	8000.284595	12.819418	-0.061955	4.816001
303.756847	8000.299563	12.824423	-0.061945	4.816006
303.433958	8000.303277	12.829427	-0.061885	4.816009
303.673691	8000.325856	12.834432	-0.061929	4.816014
303.663226	8000.349195	12.839437	-0.061927	4.816021
303.626423	8000.285455	12.844442	-0.061921	4.816003
303.652844	8000.324437	12.849447	-0.061926	4.816014
303.562072	8000.328129	12.854451	-0.061909	4.816015
303.667319	8000.361073	12.859456	-0.061929	4.816025
303.595940	8000.400400	12.864461	-0.061916	4.816036
303.641454	8000.321064	12.869466	-0.061924	4.816013
303.735208	8000.359142	12.874471	-0.061942	4.816024
303.510930	8000.317624	12.879475	-0.061900	4.816013
303.644038	8000.331834	12.884480	-0.061925	4.816016
303.656130	8000.355586	12.889485	-0.061927	4.816023
303.670459	8000.301337	12.894490	-0.061930	4.816007
303.935587	8000.366077	12.899495	-0.061979	4.816025
303.765129	8000.314853	12.904499	-0.061948	4.816010
303.781696	8000.309822	12.909504	-0.061951	4.816009
303.672799	8000.319597	12.914509	-0.061931	4.816012
303.655449	8000.229487	12.919514	-0.061928	4.815986
303.781952	8000.297030	12.924519	-0.061951	4.816005
303.897816	8000.313063	12.929523	-0.061973	4.816009
303.966495	8000.314333	12.934528	-0.061986	4.816009
303.903297	8000.329221	12.939533	-0.061974	4.816014
303.823528	8000.250796	12.944538	-0.061960	4.815991
303.763915	8000.266819	12.949543	-0.061949	4.815996
303.740446	8000.233258	12.954547	-0.061944	4.815987
303.922288	8000.223773	12.959552	-0.061978	4.815983
303.893793	8000.301304	12.964557	-0.061973	4.816006
303.691431	8000.248428	12.969562	-0.061935	4.815991
303.716063	8000.349384	12.974567	-0.061940	4.816021
303.668815	8000.343183	12.979571	-0.061932	4.816019
303.711702	8000.303354	12.984576	-0.061940	4.816007
303.916196	8000.341325	12.989581	-0.061978	4.816017
303.702229	8000.363071	12.994586	-0.061938	4.816025
303.780706	8000.342070	12.999591	-0.061953	4.816018
303.947092	8000.324818	13.004595	-0.061984	4.816012
303.975878	8000.391640	13.009600	-0.061989	4.816032
303.719266	8000.351666	13.014605	-0.061942	4.816021
303.734366	8000.309190	13.019610	-0.061945	4.816009
303.807514	8000.358651	13.024615	-0.061958	4.816023
303.792387	8000.284617	13.029619	-0.061956	4.816001
303.951564	8000.343139	13.034624	-0.061985	4.816018
303.797434	8000.372396	13.039629	-0.061957	4.816027
303.796262	8000.315724	13.044634	-0.061957	4.816010
303.881625	8000.408172	13.049639	-0.061973	4.816037
303.889514	8000.397637	13.054643	-0.061974	4.816034
303.882945	8000.370800	13.059648	-0.061973	4.816026
303.966164	8000.372336	13.064653	-0.061989	4.816026
303.730267	8000.364815	13.069658	-0.061945	4.816025
304.004294	8000.424373	13.074663	-0.061996	4.816041
303.803556	8000.371525	13.079667	-0.061959	4.816027
303.911153	8000.309363	13.084672	-0.061979	4.816008
304.098414	8000.323498	13.089677	-0.062014	4.816011
303.903076	8000.344517	13.094682	-0.061978	4.816018
303.858335	8000.370434	13.099687	-0.061969	4.816026
303.982870	8000.356692	13.104691	-0.061993	4.816021
303.949053	8000.352875	13.109696	-0.061987	4.816020
303.947533	8000.380655	13.114701	-0.061986	4.816029
303.942615	8000.271528	13.119706	-0.061986	4.815997
304.056656	8000.381608	13.124711	-0.062007	4.816028
303.965480	8000.298696	13.129715	-0.061990	4.816005
303.687574	8000.287197	13.134720	-0.061938	4.816003
303.859091	8000.353428	13.139725	-0.061970	4.816021
303.844495	8000.367070	13.144730	-0.061968	4.816025
303.827224	8000.381731	13.149735	-0.061965	4.816030
303.838881	8000.275047	13.154739	-0.061967	4.815998
303.969777	8000.307392	13.159744	-0.061991	4.816007
303.946234	8000.399982	13.164749	-0.061987	4.816034
303.891007	8000.330558	13.169754	-0.061977	4.816014
303.908292	8000.389685	13.174759	-0.061980	4.816031
303.849357	8000.339437	13.179763	-0.061970	4.816017
303.920233	8000.364268	13.184768	-0.061983	4.816024
304.008635	8000.344517	13.189773	-0.061999	4.816018
303.965384	8000.274244	13.194778	-0.061991	4.815997
303.959837	8000.337230	13.199783	-0.061991	4.816016
303.831163	8000.346641	13.204787	-0.061967	4.816019
303.931742	8000.343150	13.209792	-0.061986	4.816018
303.936068	8000.317582	13.214797	-0.061986	4.816010
303.852043	8000.279704	13.219802	-0.061971	4.816000
303.932418	8000.300431	13.224807	-0.061986	4.816005
303.902014	8000.279572	13.229811	-0.061980	4.815999
303.883152	8000.277099	13.234816	-0.061977	4.815999
304.003765	8000.321015	13.239821	-0.062000	4.816011
304.080203	8000.291424	13.244826	-0.062014	4.816002
304.072190	8000.340466	13.249831	-0.062013	4.816016
303.930540	8000.329327	13.254835	-0.061986	4.816014
303.929166	8000.307930	13.259840	-0.061986	4.816007
303.945033	8000.345650	13.264845	-0.061989	4.816018
303.838147	8000.260312	13.269850	-0.061969	4.815994
304.003391	8000.329636	13.274855	-0.062000	4.816013
303.919913	8000.330254	13.279859	-0.061985	4.816014
303.929620	8000.346479	13.284864	-0.061987	4.816019
304.164656	8000.378596	13.289869	-0.062031	4.816027
304.038148	8000.307865	13.294874	-0.062007	4.816007
303.878614	8000.309227	13.299879	-0.061978	4.816008
303.892894	8000.306293	13.304883	-0.061980	4.816007
304.056050	8000.283637	13.309888	-0.062011	4.816000
304.041312	8000.240614	13.314893	-0.062008	4.815987
303.984341	8000.190402	13.319898	-0.061998	4.815973
304.105605	8000.355137	13.324903	-0.062020	4.816020
303.988289	8000.330546	13.329907	-0.061999	4.816014
304.109040	8000.319942	13.334912	-0.062021	4.816010
304.131220	8000.297908	13.339917	-0.062025	4.816003
304.092744	8000.248035	13.344922	-0.062018	4.815989
304.028416	8000.301390	13.349927	-0.062007	4.816005
304.062737	8000.328757	13.354931	-0.062013	4.816013
303.969110	8000.287495	13.359936	-0.061996	4.816001
304.050992	8000.333909	13.364941	-0.062011	4.816014
303.768513	8000.274217	13.369946	-0.061959	4.815998
304.174161	8000.334051	13.374951	-0.062034	4.816014
304.201839	8000.335638	13.379955	-0.062039	4.816014
304.245433	8000.363175	13.384960	-0.062048	4.816022
304.034988	8000.389262	13.389965	-0.062009	4.816030
304.054605	8000.328694	13.394970	-0.062012	4.816013
304.099932	8000.400096	13.399975	-0.062021	4.816033
303.989887	8000.289042	13.404979	-0.062001	4.816001
304.145988	8000.298329	13.409984	-0.062030	4.816003
304.082465	8000.406223	13.414989	-0.062018	4.816035
303.987105	8000.358514	13.419994	-0.062000	4.816022
304.123184	8000.354605	13.424999	-0.062026	4.816020
304.218255	8000.300766	13.430003	-0.062044	4.816004
304.173840	8000.256129	13.435008	-0.062035	4.815991
304.143571	8000.331491	13.440013	-0.062030	4.816013
303.927374	8000.316847	13.445018	-0.061990	4.816010
304.161968	8000.280533	13.450023	-0.062034	4.815998
304.026171	8000.288745	13.455027	-0.062008	4.816001
304.081861	8000.296191	13.460032	-0.062019	4.816003
304.050997	8000.369403	13.465037	-0.062013	4.816025
303.996744	8000.276477	13.470042	-0.062003	4.815998
303.959229	8000.370949	13.475047	-0.061996	4.816025
304.120847	8000.353611	13.480051	-0.062027	4.816020
304.100264	8000.334000	13.485056	-0.062023	4.816014
303.951204	8000.351591	13.490061	-0.061995	4.816020
303.851481	8000.338013	13.495066	-0.061977	4.816016
304.161211	8000.369361	13.500071	-0.062035	4.816024
303.937659	8000.315026	13.505075	-0.061993	4.816009
303.902536	8000.257731	13.510080	-0.061987	4.815993
304.064802	8000.317378	13.515085	-0.062017	4.816009
303.925405	8000.268862	13.520090	-0.061991	4.815996
304.005660	8000.368701	13.525095	-0.062006	4.816025
303.869931	8000.342703	13.530099	-0.061981	4.816018
303.913712	8000.339240	13.535104	-0.061989	4.816016
304.082179	8000.393656	13.540109	-0.062021	4.816031
304.036072	8000.330814	13.545114	-0.062012	4.816013
304.240188	8000.342051	13.550119	-0.062050	4.816015
303.970913	8000.312535	13.555123	-0.062000	4.816008
303.933421	8000.325757	13.560128	-0.061993	4.816012
304.151515	8000.377875	13.565133	-0.062034	4.816026
303.892624	8000.300441	13.570138	-0.061986	4.816005
303.926361	8000.344903	13.575143	-0.061992	4.816018
304.166622	8000.336490	13.580147	-0.062037	4.816014
304.117323	8000.339873	13.585152	-0.062028	4.816015
304.035005	8000.345858	13.590157	-0.062013	4.816018
304.057402	8000.239370	13.595162	-0.062017	4.815986
304.358349	8000.347532	13.600167	-0.062073	4.816016
304.246066	8000.329447	13.605171	-0.062053	4.816012
304.210356	8000.297799	13.610176	-0.062046	4.816003
304.220497	8000.354658	13.615181	-0.062048	4.816019
304.113333	8000.318493	13.620186	-0.062028	4.816009
304.147078	8000.345850	13.625191	-0.062035	4.816017
303.982297	8000.326803	13.630195	-0.062004	4.816012
304.164662	8000.264942	13.635200	-0.062038	4.815993
304.112314	8000.308895	13.640205	-0.062028	4.816006
304.105805	8000.257470	13.645210	-0.062027	4.815991
304.245758	8000.351989	13.650215	-0.062054	4.816018
304.162217	8000.325879	13.655219	-0.062038	4.816011
304.145521	8000.280681	13.660224	-0.062035	4.815998
303.991099	8000.333454	13.665229	-0.062006	4.816014
304.230936	8000.243782	13.670234	-0.062051	4.815987
304.176024	8000.279135	13.675239	-0.062041	4.815997
304.081270	8000.297721	13.680243	-0.062024	4.816003
304.187505	8000.302887	13.685248	-0.062043	4.816004
304.118375	8000.410678	13.690253	-0.062031	4.816036
304.241592	8000.369115	13.695258	-0.062054	4.816023
304.343856	8000.356033	13.700263	-0.062073	4.816019
304.094344	8000.361091	13.705267	-0.062027	4.816022
304.109462	8000.298302	13.710272	-0.062029	4.816003
304.291371	8000.374347	13.715277	-0.062063	4.816025
304.052828	8000.284456	13.720282	-0.062019	4.816000
303.948325	8000.356318	13.725287	-0.062000	4.816021
303.920040	8000.329083	13.730291	-0.061995	4.816013
304.051112	8000.311184	13.735296	-0.062019	4.816007
304.019343	8000.358721	13.740301	-0.062013	4.816021
304.109201	8000.267368	13.745306	-0.062030	4.815994
304.214784	8000.316355	13.750311	-0.062050	4.816008
304.236605	8000.337079	13.755315	-0.062054	4.816014
304.334011	8000.289697	13.760320	-0.062072	4.816000
304.487093	8000.345970	13.765325	-0.062101	4.816015
304.110860	8000.335874	13.770330	-0.062031	4.816014
304.123763	8000.412028	13.775335	-0.062034	4.816036
303.992412	8000.325171	13.780339	-0.062009	4.816012
304.119877	8000.275134	13.785344	-0.062033	4.815996
304.188302	8000.356581	13.790349	-0.062046	4.816020
304.109405	8000.276032	13.795354	-0.062031	4.815997
304.116904	8000.316806	13.800359	-0.062033	4.816009
304.294285	8000.331829	13.805363	-0.062066	4.816012
304.193678	8000.271195	13.810368	-0.062047	4.815995
304.221386	8000.354034	13.815373	-0.062053	4.816019
304.262552	8000.312036	13.820378	-0.062060	4.816006
304.336216	8000.378612	13.825383	-0.062074	4.816025
304.396038	8000.365822	13.830387	-0.062085	4.816021
304.421968	8000.305369	13.835392	-0.062090	4.816004
304.221122	8000.388294	13.840397	-0.062053	4.816029
304.158283	8000.315523	13.845402	-0.062041	4.816008
304.485823	8000.385686	13.850407	-0.062103	4.816027
304.243545	8000.352388	13.855411	-0.062058	4.816018
304.113833	8000.291220	13.860416	-0.062034	4.816001
304.136583	8000.353655	13.865421	-0.062038	4.816019
304.212193	8000.246005	13.870426	-0.062052	4.815987
304.133610	8000.270233	13.875431	-0.062038	4.815995
304.072920	8000.272338	13.880435	-0.062026	4.815996
304.254024	8000.301328	13.885440	-0.062060	4.816003
304.366852	8000.368622	13.890445	-0.062081	4.816022
304.253428	8000.362277	13.895450	-0.062060	4.816021
304.251242	8000.393251	13.900455	-0.062060	4.816030
304.148356	8000.399928	13.905459	-0.062041	4.816033
304.066596	8000.358883	13.910464	-0.062026	4.816021
304.254635	8000.390138	13.915469	-0.062061	4.816029
304.133520	8000.350510	13.920474	-0.062039	4.816018
304.251711	8000.345204	13.925479	-0.062061	4.816016
304.158166	8000.370227	13.930483	-0.062043	4.816024
304.290952	8000.311734	13.935488	-0.062068	4.816006
304.390544	8000.350989	13.940493	-0.062087	4.816017
304.291726	8000.348119	13.945498	-0.062069	4.816017
304.389465	8000.385202	13.950503	-0.062087	4.816027
304.364140	8000.387956	13.955507	-0.062082	4.816028
304.256397	8000.345365	13.960512	-0.062062	4.816016
304.369491	8000.359210	13.965517	-0.062083	4.816020
304.433208	8000.333661	13.970522	-0.062095	4.816012
304.410154	8000.383497	13.975527	-0.062091	4.816026
304.141522	8000.334748	13.980531	-0.062041	4.816014
304.182654	8000.324822	13.985536	-0.062049	4.816010
304.065570	8000.368657	13.990541	-0.062027	4.816024
304.072983	8000.291829	13.995546	-0.062029	4.816001
304.161224	8000.295596	14.000551	-0.062045	4.816002
304.133118	8000.351753	14.005555	-0.062040	4.816019
304.029970	8000.253655	14.010560	-0.062021	4.815990
304.154928	8000.336138	14.015565	-0.062045	4.816014
304.097452	8000.265604	14.020570	-0.062034	4.815994
304.277403	8000.294573	14.025575	-0.062068	4.816001
304.114610	8000.343984	14.030579	-0.062037	4.816016
304.223512	8000.305366	14.035584	-0.062058	4.816005
304.214163	8000.376835	14.040589	-0.062056	4.816025
304.042406	8000.352314	14.045594	-0.062024	4.816019
304.182079	8000.295016	14.050599	-0.062050	4.816002
304.255669	8000.360522	14.055603	-0.062064	4.816020
304.211089	8000.265635	14.060608	-0.062056	4.815993
304.312432	8000.380829	14.065613	-0.062075	4.816026
304.260992	8000.359583	14.070618	-0.062066	4.816020
304.456479	8000.358902	14.075623	-0.062102	4.816019
304.281036	8000.347143	14.080627	-0.062069	4.816016
304.229566	8000.371868	14.085632	-0.062060	4.816024
304.245695	8000.409593	14.090637	-0.062063	4.816035
304.290349	8000.336655	14.095642	-0.062072	4.816013
304.220283	8000.330035	14.100647	-0.062059	4.816012
304.248201	8000.353009	14.105651	-0.062064	4.816018
304.156172	8000.319259	14.110656	-0.062047	4.816009
304.063772	8000.346441	14.115661	-0.062030	4.816017
304.307823	8000.265399	14.120666	-0.062075	4.815992
304.274085	8000.306486	14.125671	-0.062069	4.816005
304.236103	8000.317560	14.130675	-0.062062	4.816008
304.272441	8000.262644	14.135680	-0.062069	4.815992
304.451877	8000.281982	14.140685	-0.062103	4.815996
304.215096	8000.272305	14.145690	-0.062059	4.815995
304.350143	8000.309003	14.150695	-0.062084	4.816005
304.380938	8000.355550	14.155699	-0.062090	4.816018
304.316453	8000.334065	14.160704	-0.062078	4.816012
304.337241	8000.372945	14.165709	-0.062082	4.816024
304.446705	8000.346097	14.170714	-0.062102	4.816015
304.472434	8000.365824	14.175719	-0.062107	4.816021
304.375128	8000.342668	14.180723	-0.062089	4.816015
304.477616	8000.295379	14.185728	-0.062108	4.816000
304.578233	8000.371004	14.190733	-0.062127	4.816022
304.210140	8000.318293	14.195738	-0.062059	4.816008
304.108593	8000.331409	14.200743	-0.062040	4.816013
304.253917	8000.321255	14.205747	-0.062067	4.816009
304.404338	8000.306918	14.210752	-0.062095	4.816004
304.362595	8000.329684	14.215757	-0.062088	4.816011
304.179865	8000.311377	14.220762	-0.062054	4.816006
304.308374	8000.352231	14.225767	-0.062078	4.816018
304.261893	8000.351390	14.230771	-0.062069	4.816018
304.179414	8000.313539	14.235776	-0.062054	4.816007
304.329072	8000.322708	14.240781	-0.062082	4.816009
304.269586	8000.279933	14.245786	-0.062071	4.815997
304.339942	8000.348587	14.250791	-0.062084	4.816016
304.431619	8000.358832	14.255795	-0.062101	4.816019
304.465512	7999.265804	14.260800	-0.062107	4.815700

304.432736	7996.097968	14.265805	-0.062099	4.814774
304.307765	7990.610330	14.270810	-0.062072	4.813172
304.321719	7983.956442	14.275815	-0.062071	4.811227
304.239656	7976.636302	14.280819	-0.062051	4.809087
304.176030	7969.003928	14.285824	-0.062034	4.806855
304.259001	7961.216628	14.290829	-0.062044	4.804576
304.038256	7953.346760	14.295834	-0.061998	4.802273
303.975138	7945.397132	14.300839	-0.061982	4.799944
303.893900	7937.467063	14.305843	-0.061961	4.797621
303.939098	7929.386498	14.310848	-0.061965	4.795251
304.098962	7921.389468	14.315853	-0.061989	4.792904
303.827518	7913.356343	14.320858	-0.061934	4.790548
303.936149	7905.431159	14.325863	-0.061949	4.788220
303.996802	7897.433606	14.330867	-0.061955	4.785870
303.559792	7889.383345	14.335872	-0.061868	4.783506
303.674970	7881.398827	14.340877	-0.061885	4.781157
303.680190	7873.400610	14.345882	-0.061881	4.778804
303.710474	7865.412018	14.350887	-0.061881	4.776452
303.635334	7857.416254	14.355891	-0.061862	4.774097
303.555976	7849.360857	14.360896	-0.061842	4.771724
303.488458	7841.380611	14.365901	-0.061825	4.769371
303.141485	7833.354850	14.370906	-0.061755	4.767006
303.307099	7825.346770	14.375911	-0.061781	4.764642
303.249483	7817.471653	14.380915	-0.061765	4.762317
303.179501	7809.349830	14.385920	-0.061747	4.759918
303.293300	7801.415201	14.390925	-0.061763	4.757572
303.117546	7793.378216	14.395930	-0.061725	4.755196
303.067025	7785.324807	14.400935	-0.061710	4.752814
302.990659	7777.335237	14.405939	-0.061691	4.750449
302.969574	7769.299795	14.410944	-0.061682	4.748070
303.040690	7761.336969	14.415949	-0.061690	4.745710
302.729590	7753.316526	14.420954	-0.061627	4.743334
302.886797	7745.330104	14.425959	-0.061651	4.740964
302.990333	7737.385902	14.430963	-0.061665	4.738607
302.698222	7729.284342	14.435968	-0.061606	4.736202
302.930902	7721.351730	14.440973	-0.061644	4.733845
302.831340	7713.275340	14.445978	-0.061620	4.731445
302.582954	7705.308510	14.450983	-0.061569	4.729077
302.525074	7697.306939	14.455987	-0.061553	4.726697
302.587849	7689.279265	14.460992	-0.061560	4.724308
302.782989	7681.360797	14.465997	-0.061591	4.721949
302.546696	7673.314995	14.471002	-0.061542	4.719552
302.575058	7665.351455	14.476007	-0.061542	4.717178
302.619975	7657.306270	14.481011	-0.061545	4.714779
302.452085	7649.282969	14.486016	-0.061509	4.712385
302.554856	7641.265362	14.491021	-0.061523	4.709991
302.334671	7633.310424	14.496026	-0.061477	4.707616
302.348097	7625.272965	14.501031	-0.061474	4.705214
302.192426	7617.321603	14.506035	-0.061440	4.702837
302.169345	7609.295159	14.511040	-0.061431	4.700435
302.331595	7601.327608	14.516045	-0.061456	4.698050
302.349528	7593.297175	14.521050	-0.061454	4.695645
302.079401	7585.307040	14.526055	-0.061399	4.693252
302.058235	7577.250203	14.531059	-0.061390	4.690837
301.991172	7569.297076	14.536064	-0.061372	4.688452
301.826736	7561.297364	14.541069	-0.061336	4.686051
301.804320	7553.320548	14.546074	-0.061327	4.683657
301.895886	7545.300857	14.551079	-0.061339	4.681247
301.715409	7537.325934	14.556083	-0.061300	4.678851
301.733420	7529.310861	14.561088	-0.061299	4.676441
301.785855	7521.228566	14.566093	-0.061303	4.674009
301.565091	7513.139376	14.571098	-0.061257	4.671574
301.691286	7505.150970	14.576103	-0.061275	4.669168
301.732718	7497.203418	14.581107	-0.061278	4.666773
301.680352	7489.205554	14.586112	-0.061263	4.664362
301.745767	7481.322205	14.591117	-0.061270	4.661984
301.674196	7473.242508	14.596122	-0.061252	4.659546
301.536228	7465.285599	14.601127	-0.061221	4.657144
301.413791	7457.232723	14.606131	-0.061193	4.654711
301.269055	7449.210852	14.611136	-0.061161	4.652286
301.392194	7441.174871	14.616141	-0.061179	4.649856
301.216330	7433.229390	14.621146	-0.061141	4.647452
301.266415	7425.174628	14.626151	-0.061145	4.645013
301.253840	7417.275302	14.631155	-0.061138	4.642621
301.070238	7409.205342	14.636160	-0.061098	4.640175
301.097531	7401.270194	14.641165	-0.061098	4.637769
301.081172	7393.202178	14.646170	-0.061090	4.635321
301.249859	7385.184294	14.651175	-0.061117	4.632888
300.992679	7377.170268	14.656179	-0.061064	4.630454
301.000059	7369.168525	14.661184	-0.061060	4.628023
300.986587	7361.203789	14.666189	-0.061052	4.625601
300.862234	7353.226539	14.671194	-0.061024	4.623175
300.790407	7345.212634	14.676199	-0.061006	4.620736
300.820290	7337.241140	14.681203	-0.061006	4.618308
300.859705	7329.166282	14.686208	-0.061008	4.615848
300.869865	7321.201135	14.691213	-0.061005	4.613420
300.716836	7313.138618	14.696218	-0.060971	4.610961
300.826062	7305.177994	14.701223	-0.060987	4.608532
300.645433	7297.163949	14.706227	-0.060948	4.606085
300.530051	7289.161456	14.711232	-0.060921	4.603641
300.539311	7281.183787	14.716237	-0.060918	4.601203
300.543715	7273.194017	14.721242	-0.060914	4.598759
300.392569	7265.184979	14.726247	-0.060880	4.596309
300.406276	7257.156860	14.731251	-0.060878	4.593851
300.190700	7249.090245	14.736256	-0.060833	4.591380
300.339588	7241.122705	14.741261	-0.060855	4.588939
300.272437	7233.067831	14.746266	-0.060838	4.586469
300.467007	7225.147397	14.751271	-0.060869	4.584039
300.117524	7217.150180	14.756275	-0.060799	4.581584
300.004717	7209.137851	14.761280	-0.060772	4.579124
300.114100	7201.155011	14.766285	-0.060788	4.576671
300.012310	7193.108691	14.771290	-0.060764	4.574197
299.849467	7185.088175	14.776295	-0.060728	4.571729
299.869164	7177.100132	14.781299	-0.060727	4.569271
299.805242	7169.088175	14.786304	-0.060710	4.566803
299.722601	7161.147478	14.791309	-0.060689	4.564357
299.614779	7153.155455	14.796314	-0.060664	4.561893
299.734593	7145.133827	14.801319	-0.060681	4.559419
299.643640	7137.194966	14.806323	-0.060659	4.556969
299.488639	7129.112022	14.811328	-0.060625	4.554472
299.608717	7121.097369	14.816333	-0.060642	4.551996
299.474292	7113.078800	14.821338	-0.060612	4.549518
299.624060	7105.122188	14.826343	-0.060635	4.547057
299.762637	7097.084145	14.831347	-0.060656	4.544569
299.440192	7089.123834	14.836352	-0.060591	4.542104
299.244738	7081.109024	14.841357	-0.060549	4.539621
299.411298	7073.152503	14.846362	-0.060575	4.537155
299.438677	7065.103260	14.851367	-0.060575	4.534659
299.389553	7057.122174	14.856371	-0.060561	4.532182
299.297394	7049.019026	14.861376	-0.060539	4.529666
299.247838	7041.124161	14.866381	-0.060524	4.527213
299.195941	7033.081988	14.871386	-0.060509	4.524714
298.929647	7025.156863	14.876391	-0.060455	4.522248
298.841086	7017.155921	14.881395	-0.060433	4.519759
299.054845	7009.157655	14.886400	-0.060468	4.517269
298.938489	7001.133665	14.891405	-0.060441	4.514769
298.873798	6993.019721	14.896410	-0.060424	4.512240
298.911130	6985.015786	14.901415	-0.060426	4.509744
298.919202	6977.048479	14.906419	-0.060422	4.507258
298.765033	6969.034700	14.911424	-0.060388	4.504756
298.773829	6961.122211	14.916429	-0.060385	4.502284
298.738399	6953.068596	14.921434	-0.060373	4.499767
298.811924	6945.083572	14.926439	-0.060382	4.497270
298.715898	6937.082312	14.931443	-0.060359	4.494766
298.636003	6929.045554	14.936448	-0.060339	4.492249
298.543316	6921.063259	14.941453	-0.060316	4.489749
298.383417	6913.062109	14.946458	-0.060282	4.487240
298.540472	6905.051889	14.951463	-0.060306	4.484729
298.430099	6897.085208	14.956467	-0.060280	4.482229
298.272697	6889.051862	14.961472	-0.060246	4.479706
298.328694	6881.134456	14.966477	-0.060251	4.477219
298.248891	6873.048908	14.971482	-0.060231	4.474678
298.041054	6865.016835	14.976487	-0.060187	4.472151
298.075084	6857.050550	14.981491	-0.060188	4.469644
298.085558	6848.995777	14.986496	-0.060185	4.467108
298.360351	6841.051926	14.991501	-0.060231	4.464607
298.205521	6833.062338	14.996506	-0.060197	4.462088
298.281727	6825.037328	15.001511	-0.060206	4.459557
298.001031	6817.035459	15.006515	-0.060149	4.457031
297.844774	6809.041849	15.011520	-0.060115	4.454507
297.971577	6800.999354	15.016525	-0.060133	4.451966
297.978199	6792.997306	15.021530	-0.060130	4.449437
297.781583	6785.014949	15.026535	-0.060088	4.446911
297.645457	6777.010871	15.031539	-0.060057	4.444378
297.695596	6769.045703	15.036544	-0.060062	4.441856
297.671085	6761.038653	15.041549	-0.060052	4.439319
297.524941	6753.067209	15.046554	-0.060020	4.436791
297.608935	6744.980443	15.051559	-0.060030	4.434227
297.621216	6736.963150	15.056563	-0.060027	4.431682
297.361073	6728.964740	15.061568	-0.059974	4.429141
297.465281	6721.000707	15.066573	-0.059988	4.426611
297.380483	6712.965135	15.071578	-0.059967	4.424056
297.270932	6704.980689	15.076583	-0.059942	4.421516
297.229462	6696.991139	15.081587	-0.059929	4.418973
297.336099	6688.976745	15.086592	-0.059944	4.416421
297.420856	6680.971170	15.091597	-0.059954	4.413870
297.077796	6672.957625	15.096602	-0.059885	4.411313
297.196007	6664.982393	15.101607	-0.059902	4.408770
297.242362	6656.975611	15.106611	-0.059906	4.406214
297.131127	6648.963072	15.111616	-0.059880	4.403654
297.147392	6641.012923	15.116621	-0.059878	4.401113
297.074636	6633.024784	15.121626	-0.059859	4.398559
296.874030	6624.984746	15.126631	-0.059817	4.395985
296.648825	6616.959634	15.131635	-0.059770	4.393415
296.630739	6608.928281	15.136640	-0.059761	4.390842
296.692800	6601.007492	15.141645	-0.059768	4.388304
296.802549	6592.934796	15.146650	-0.059783	4.385715
296.688925	6584.998840	15.151655	-0.059757	4.383168
296.646529	6577.004170	15.156659	-0.059744	4.380601
296.462243	6569.032114	15.161664	-0.059704	4.378038
296.558536	6561.024164	15.166669	-0.059717	4.375465
296.453492	6552.949607	15.171674	-0.059692	4.372867
296.334703	6544.954805	15.176679	-0.059665	4.370293
296.370401	6537.013444	15.181683	-0.059667	4.367736
296.237535	6528.953778	15.186688	-0.059637	4.365138
296.430768	6520.989001	15.191693	-0.059668	4.362571
296.335199	6512.969219	15.196698	-0.059645	4.359983
296.114020	6505.043548	15.201703	-0.059599	4.357424
296.105052	6496.974752	15.206707	-0.059592	4.354817
295.870873	6488.886012	15.211712	-0.059543	4.352202
296.038940	6480.918219	15.216717	-0.059569	4.349626
295.967759	6472.944193	15.221722	-0.059551	4.347045
295.977129	6464.912663	15.226727	-0.059548	4.344445
295.888229	6456.993823	15.231731	-0.059526	4.341879
295.938401	6448.951820	15.236736	-0.059530	4.339273
295.865378	6440.995013	15.241741	-0.059511	4.336691
295.683356	6432.974952	15.246746	-0.059472	4.334087
295.603359	6424.929866	15.251751	-0.059452	4.331474
295.600013	6416.998574	15.256755	-0.059447	4.328897
295.475590	6408.921872	15.261760	-0.059418	4.326270
295.412040	6400.983180	15.266765	-0.059402	4.323687
295.305457	6392.959083	15.271770	-0.059377	4.321074
295.621781	6384.968327	15.276775	-0.059430	4.318473
295.553093	6376.993345	15.281779	-0.059413	4.315874
295.296410	6368.934415	15.286784	-0.059360	4.313244
295.373178	6360.913445	15.291789	-0.059369	4.310627
295.456818	6352.927760	15.296794	-0.059379	4.308020
295.262911	6344.942507	15.301799	-0.059338	4.305410
295.237562	6336.972746	15.306803	-0.059328	4.302804
295.212477	6328.920046	15.311808	-0.059318	4.300170
295.165507	6320.982450	15.316813	-0.059305	4.297571
295.138429	6312.945356	15.321818	-0.059294	4.294939
295.150978	6304.926579	15.326823	-0.059292	4.292311
295.020939	6296.919840	15.331827	-0.059262	4.289684
294.940430	6288.931171	15.336832	-0.059242	4.287063
295.124686	6280.941165	15.341837	-0.059271	4.284441
294.888481	6272.945113	15.346842	-0.059222	4.281812
294.811610	6264.927456	15.351847	-0.059203	4.279176
294.818571	6256.963036	15.356851	-0.059199	4.276556
294.833449	6248.899946	15.361856	-0.059197	4.273902
294.787846	6240.893583	15.366861	-0.059183	4.271265
294.613688	6232.917165	15.371866	-0.059146	4.268635
294.498667	6224.848666	15.376871	-0.059119	4.265974
294.630767	6216.932260	15.381875	-0.059139	4.263363
294.408013	6208.887879	15.386880	-0.059092	4.260705
294.558632	6200.979817	15.391885	-0.059115	4.258094
294.548470	6192.862603	15.396890	-0.059108	4.255411
294.501341	6184.888298	15.401895	-0.059094	4.252772
294.414560	6176.857771	15.406899	-0.059073	4.250114
294.346323	6168.895903	15.411904	-0.059055	4.247476
294.239944	6160.903301	15.416909	-0.059030	4.244827
294.255580	6152.945414	15.421914	-0.059028	4.242188
294.216103	6144.925302	15.426919	-0.059015	4.239526
294.152735	6136.994561	15.431923	-0.058999	4.236893
293.998828	6128.935985	15.436928	-0.058965	4.234214
294.048521	6120.925786	15.441933	-0.058969	4.231552
293.981650	6112.895704	15.446938	-0.058951	4.228880
293.988833	6104.935235	15.451943	-0.058948	4.226230
294.032834	6096.949677	15.456947	-0.058951	4.223571
294.015825	6088.895015	15.461952	-0.058942	4.220886
293.945548	6080.977097	15.466957	-0.058924	4.218245
293.904327	6072.916502	15.471962	-0.058911	4.215555
294.008238	6064.887722	15.476967	-0.058926	4.212875
293.742487	6056.912146	15.481971	-0.058871	4.210207
293.569051	6048.924099	15.486976	-0.058834	4.207535
293.986417	6040.949886	15.491981	-0.058906	4.204871
293.627114	6032.981265	15.496986	-0.058834	4.202200
293.501060	6024.958715	15.501991	-0.058806	4.199511
293.534324	6016.964498	15.506995	-0.058807	4.196832
293.357750	6008.877524	15.512000	-0.058769	4.194118
293.384816	6000.850097	15.517005	-0.058769	4.191424
293.285202	5992.863311	15.522010	-0.058745	4.188740
293.238078	5984.894930	15.527015	-0.058731	4.186062
293.467093	5976.953720	15.532019	-0.058769	4.183394
293.343111	5968.900534	15.537024	-0.058741	4.180683
293.353445	5960.945729	15.542029	-0.058737	4.178005
293.215330	5952.888645	15.547034	-0.058707	4.175288
293.004163	5944.909550	15.552039	-0.058662	4.172596
293.149229	5936.926129	15.557043	-0.058684	4.169904
293.098186	5928.909760	15.562048	-0.058669	4.167197
293.186607	5920.890408	15.567053	-0.058681	4.164489
292.952060	5912.921870	15.572058	-0.058632	4.161793
292.952253	5904.892762	15.577063	-0.058627	4.159077
292.826733	5896.956969	15.582067	-0.058599	4.156390
292.824113	5888.885904	15.587072	-0.058593	4.153656
292.920573	5880.874863	15.592077	-0.058606	4.150942
292.791318	5872.891343	15.597082	-0.058577	4.148233
292.724738	5864.867755	15.602087	-0.058559	4.145510
292.625374	5856.944334	15.607091	-0.058536	4.142818
292.610362	5848.895560	15.612096	-0.058528	4.140083
292.703578	5840.935591	15.617101	-0.058540	4.137377
292.431943	5832.882433	15.622106	-0.058484	4.134634
292.418850	5824.854161	15.627111	-0.058477	4.131900
292.267115	5816.908431	15.632115	-0.058443	4.129191
292.169239	5808.889195	15.637120	-0.058420	4.126456
292.236322	5800.903336	15.642125	-0.058427	4.123733
292.344405	5792.887448	15.647130	-0.058442	4.120997
292.231451	5784.902109	15.652135	-0.058416	4.118268
292.291985	5776.901271	15.657139	-0.058422	4.115534
292.126696	5768.868279	15.662144	-0.058386	4.112784
292.129449	5760.871097	15.667149	-0.058382	4.110047
292.027745	5752.860288	15.672154	-0.058358	4.107301
292.092618	5744.876990	15.677159	-0.058365	4.104566
292.067507	5736.906869	15.682163	-0.058355	4.101832
291.732211	5728.905403	15.687168	-0.058288	4.099082
291.854500	5720.947804	15.692173	-0.058305	4.096350
291.963333	5712.882460	15.697178	-0.058320	4.093580
291.775017	5704.879123	15.702183	-0.058280	4.090825
291.708718	5696.940117	15.707187	-0.058263	4.088092
291.505439	5688.900205	15.712192	-0.058220	4.085320
291.525649	5680.990409	15.717197	-0.058218	4.082595
291.673769	5672.928016	15.722202	-0.058241	4.079817
291.541997	5664.975049	15.727207	-0.058211	4.077070
291.566456	5656.936467	15.732211	-0.058211	4.074295
291.308828	5648.900838	15.737216	-0.058158	4.071515
291.436647	5640.912533	15.742221	-0.058176	4.068754
291.396314	5632.927222	15.747226	-0.058164	4.065991
291.145105	5624.973757	15.752231	-0.058112	4.063233
291.155417	5616.957730	15.757235	-0.058109	4.060456
291.264981	5608.975617	15.762240	-0.058124	4.057690
291.084641	5600.953912	15.767245	-0.058085	4.054904
290.854588	5592.973971	15.772250	-0.058037	4.052130
290.995705	5584.883905	15.777255	-0.058058	4.049321
291.012649	5576.926550	15.782259	-0.058057	4.046555
290.830762	5568.935255	15.787264	-0.058018	4.043772
290.850013	5560.962764	15.792269	-0.058016	4.040997
290.828614	5552.994746	15.797274	-0.058007	4.038220
290.693792	5544.932213	15.802279	-0.057977	4.035407
290.586805	5536.858994	15.807283	-0.057952	4.032589
290.619172	5528.836568	15.812288	-0.057953	4.029789
290.684909	5520.883512	15.817293	-0.057960	4.027011
290.588716	5512.884768	15.822298	-0.057937	4.024213
290.472796	5504.908531	15.827303	-0.057910	4.021421
290.517918	5496.947043	15.832307	-0.057913	4.018634
290.414665	5488.914601	15.837312	-0.057889	4.015818
290.361696	5480.931960	15.842317	-0.057874	4.013019
290.284649	5472.875015	15.847322	-0.057855	4.010191
290.188290	5464.931304	15.852327	-0.057832	4.007400
290.142956	5456.900335	15.857331	-0.057818	4.004578
290.066811	5448.907476	15.862336	-0.057799	4.001767
290.167283	5440.910698	15.867341	-0.057812	3.998955
290.084657	5432.950679	15.872346	-0.057792	3.996151
290.134855	5424.915964	15.877351	-0.057796	3.993321
290.317333	5416.910221	15.882355	-0.057825	3.990501
290.114103	5408.908829	15.887360	-0.057782	3.987675
290.148361	5400.862706	15.892365	-0.057783	3.984834
289.899291	5392.964116	15.897370	-0.057732	3.982040
289.956792	5384.938948	15.902375	-0.057737	3.979203
289.928421	5376.971924	15.907379	-0.057727	3.976383
289.757297	5368.906952	15.912384	-0.057690	3.973525
289.708827	5360.918832	15.917389	-0.057676	3.970694
289.700947	5352.928395	15.922394	-0.057669	3.967860
289.664012	5344.908090	15.927399	-0.057657	3.965013
289.849209	5336.986018	15.932403	-0.057687	3.962203
289.723675	5328.979559	15.937408	-0.057658	3.959356
289.464175	5321.007169	15.942413	-0.057605	3.956517
289.273751	5312.969826	15.947418	-0.057564	3.953653
289.343986	5304.906738	15.952423	-0.057572	3.950783
289.329925	5296.945452	15.957427	-0.057565	3.947945
289.120179	5288.919643	15.962432	-0.057520	3.945079
289.405181	5280.978283	15.967437	-0.057568	3.942250
289.355616	5272.988758	15.972442	-0.057554	3.939395
289.115417	5264.995953	15.977447	-0.057504	3.936534
289.143912	5256.994249	15.982451	-0.057504	3.933673
289.142957	5248.956208	15.987456	-0.057499	3.930795
289.070753	5241.005094	15.992461	-0.057481	3.927946
288.927662	5232.984924	15.997466	-0.057449	3.925068
288.970721	5225.021527	16.002471	-0.057452	3.922212
289.047871	5216.996159	16.007475	-0.057461	3.919333
288.814055	5209.028642	16.012480	-0.057412	3.916466
288.723436	5201.001744	16.017485	-0.057390	3.913578
288.798521	5192.975096	16.022490	-0.057399	3.910692
288.683723	5185.000325	16.027495	-0.057373	3.907818
288.942463	5176.979659	16.032499	-0.057416	3.904933
288.895086	5169.001141	16.037504	-0.057402	3.902055
288.796736	5161.005191	16.042509	-0.057379	3.899168
288.740333	5153.015657	16.047514	-0.057363	3.896282
288.535291	5144.993082	16.052519	-0.057320	3.893378
288.675692	5136.957902	16.057523	-0.057341	3.890475
288.369848	5129.000060	16.062528	-0.057279	3.887589
288.564472	5120.997266	16.067533	-0.057310	3.884694
288.538583	5113.039417	16.072538	-0.057300	3.881809
288.304460	5105.032161	16.077543	-0.057251	3.878900
288.447253	5097.017225	16.082547	-0.057273	3.875993
288.286503	5088.840432	16.087552	-0.057238	3.873019
288.461919	5080.816140	16.092557	-0.057265	3.870105
288.355418	5072.896006	16.097562	-0.057240	3.867221
288.270428	5064.900118	16.102567	-0.057219	3.864308
288.341312	5056.988458	16.107571	-0.057227	3.861427
288.159794	5048.981566	16.112576	-0.057188	3.858503
288.007168	5040.983545	16.117581	-0.057155	3.855581
288.074322	5033.014797	16.122586	-0.057162	3.852672
287.803609	5024.974770	16.127591	-0.057107	3.849728
287.857449	5017.037649	16.132595	-0.057112	3.846826
287.809822	5009.010601	16.137600	-0.057098	3.843887
287.770607	5001.042927	16.142605	-0.057085	3.840967
287.822720	4993.030336	16.147610	-0.057090	3.838030
287.774771	4985.035348	16.152615	-0.057076	3.835096
287.943803	4977.038716	16.157619	-0.057102	3.832163
287.804727	4969.016888	16.162624	-0.057071	3.829212
287.534393	4961.033254	16.167629	-0.057016	3.826271
287.520906	4953.065223	16.172634	-0.057008	3.823338
287.520811	4945.066131	16.177639	-0.057003	3.820392
287.498309	4937.083794	16.182643	-0.056994	3.817449
287.177496	4929.083923	16.187648	-0.056929	3.814491
287.245996	4921.067423	16.192653	-0.056937	3.811533
287.128844	4913.098968	16.197658	-0.056910	3.808587
287.223082	4905.079058	16.202663	-0.056922	3.805623
287.085555	4897.130962	16.207667	-0.056892	3.802679
287.167355	4889.079536	16.212672	-0.056902	3.799699
287.221464	4881.117675	16.217677	-0.056907	3.796750
287.111902	4873.083978	16.222682	-0.056881	3.793767
286.982022	4865.046907	16.227687	-0.056852	3.790781
286.925178	4857.085889	16.232691	-0.056836	3.787823
286.742057	4849.057942	16.237696	-0.056797	3.784834
286.794520	4841.132442	16.242701	-0.056802	3.781886
286.648756	4833.104956	16.247706	-0.056769	3.778894
286.620068	4825.093717	16.252711	-0.056759	3.775907
286.700714	4817.102422	16.257715	-0.056769	3.772929
286.506538	4809.066899	16.262720	-0.056728	3.769925
286.527825	4801.126075	16.267725	-0.056726	3.766959
286.507571	4793.100501	16.272730	-0.056718	3.763958
286.385961	4785.133317	16.277735	-0.056690	3.760975
286.463052	4777.162185	16.282739	-0.056699	3.757991
286.576033	4769.109408	16.287744	-0.056715	3.754976
286.498055	4761.116263	16.292749	-0.056695	3.751977
286.324157	4753.095490	16.297754	-0.056658	3.748962
286.238077	4745.081696	16.302759	-0.056637	3.745950
286.451166	4737.139877	16.307763	-0.056671	3.742969
286.233378	4729.106402	16.312768	-0.056626	3.739941
286.289420	4721.153791	16.317773	-0.056631	3.736948
286.314716	4713.160581	16.322778	-0.056631	3.733936
286.156851	4705.102455	16.327783	-0.056596	3.730893
286.234417	4697.167755	16.332787	-0.056605	3.727899
285.973436	4689.109397	16.337792	-0.056552	3.724849
285.858935	4681.221905	16.342797	-0.056525	3.721864
285.883979	4673.188519	16.347802	-0.056525	3.718825
285.801161	4665.193222	16.352807	-0.056504	3.715795
285.982186	4657.116157	16.357811	-0.056533	3.712738
285.739338	4649.086569	16.362816	-0.056483	3.709686
285.702072	4641.145960	16.367821	-0.056471	3.706670
285.774181	4633.161318	16.372826	-0.056479	3.703638
285.408254	4625.198948	16.377831	-0.056406	3.700602
285.567885	4617.208682	16.382835	-0.056430	3.697564
285.459953	4609.188093	16.387840	-0.056405	3.694507
285.426786	4601.176730	16.392845	-0.056394	3.691452
285.415465	4593.195959	16.397850	-0.056387	3.688407
285.264086	4585.223545	16.402855	-0.056353	3.685359
285.441134	4577.249437	16.407859	-0.056381	3.682316
285.304695	4569.222404	16.412864	-0.056351	3.679242
285.160543	4561.280913	16.417869	-0.056319	3.676198
285.392345	4553.254526	16.422874	-0.056357	3.673129
285.220528	4545.230474	16.427879	-0.056320	3.670048
285.120038	4537.262189	16.432883	-0.056296	3.666988
284.882922	4529.234120	16.437888	-0.056247	3.663898
285.088404	4521.242712	16.442893	-0.056280	3.660831
284.877572	4513.280051	16.447898	-0.056235	3.657762
284.872383	4505.231781	16.452903	-0.056229	3.654663
285.037610	4497.281733	16.457907	-0.056255	3.651604
284.758817	4489.245226	16.462912	-0.056198	3.648497
284.779152	4481.247213	16.467917	-0.056197	3.645410
284.629208	4473.306283	16.472922	-0.056164	3.642338
284.624672	4465.280734	16.477927	-0.056158	3.639234
284.558847	4457.325884	16.482931	-0.056140	3.636153
284.454133	4449.262042	16.487936	-0.056116	3.633027
284.606336	4441.215751	16.492941	-0.056139	3.629912
284.536857	4433.271972	16.497946	-0.056121	3.626827
284.479338	4425.241755	16.502951	-0.056105	3.623707
284.267362	4417.291789	16.507955	-0.056061	3.620611
284.332813	4409.300606	16.512960	-0.056068	3.617504
284.293366	4401.324362	16.517965	-0.056055	3.614398
284.223304	4393.307485	16.522970	-0.056037	3.611272
284.123961	4385.333238	16.527975	-0.056014	3.608159
284.101009	4377.337384	16.532979	-0.056004	3.605037
284.048367	4369.380911	16.537984	-0.055989	3.601927
284.132252	4361.362659	16.542989	-0.056000	3.598793
283.972408	4353.375769	16.547994	-0.055965	3.595663
283.874377	4345.370816	16.552999	-0.055942	3.592524
283.882362	4337.368555	16.558003	-0.055938	3.589387
284.015573	4329.351640	16.563008	-0.055958	3.586245
283.896874	4321.398638	16.568013	-0.055930	3.583118
283.835181	4313.385839	16.573018	-0.055914	3.579966
283.853623	4305.397371	16.578023	-0.055912	3.576824
284.028693	4297.404631	16.583027	-0.055940	3.573681
283.672280	4289.396295	16.588032	-0.055868	3.570514
283.667458	4281.422751	16.593037	-0.055862	3.567369
283.681971	4273.426392	16.598042	-0.055860	3.564212
283.559719	4265.432868	16.603047	-0.055832	3.561049
283.544692	4257.478118	16.608051	-0.055824	3.557902
283.471607	4249.419592	16.613056	-0.055805	3.554709
283.327790	4241.367240	16.618061	-0.055773	3.551514
283.292455	4233.376372	16.623066	-0.055762	3.548344
283.261164	4225.375076	16.628071	-0.055751	3.545167
283.419753	4217.443098	16.633075	-0.055775	3.542020
282.985653	4209.467146	16.638080	-0.055689	3.538835
282.967232	4201.441774	16.643085	-0.055681	3.535640
283.064964	4193.426752	16.648090	-0.055694	3.532450
282.941478	4185.419047	16.653095	-0.055666	3.529253
283.073993	4177.458878	16.658099	-0.055685	3.526079
282.993206	4169.474992	16.663104	-0.055665	3.522887
282.919718	4161.493931	16.668109	-0.055646	3.519694
282.875636	4153.517150	16.673114	-0.055633	3.516500
282.802102	4145.474311	16.678119	-0.055614	3.513276
282.864717	4137.492368	16.683123	-0.055621	3.510078
282.498074	4129.517717	16.688128	-0.055548	3.506866
282.734489	4121.520805	16.693133	-0.055586	3.503661
282.727386	4113.510168	16.698138	-0.055580	3.500440
282.590273	4105.548684	16.703143	-0.055549	3.497232
282.593891	4097.573673	16.708147	-0.055545	3.494020
282.364874	4089.559705	16.713152	-0.055497	3.490781
282.528093	4081.562385	16.718157	-0.055523	3.487559
282.490682	4073.573262	16.723162	-0.055510	3.484331
282.351863	4065.604852	16.728167	-0.055480	3.481105
282.380296	4057.636261	16.733171	-0.055480	3.477881
282.127066	4049.616163	16.738176	-0.055427	3.474625
281.946713	4041.583375	16.743181	-0.055389	3.471362
282.091853	4033.564198	16.748186	-0.055411	3.468113
281.920789	4025.564304	16.753191	-0.055374	3.464858
281.930286	4017.631445	16.758195	-0.055370	3.461633
281.922103	4009.637600	16.763200	-0.055364	3.458379
281.780042	4001.637387	16.768205	-0.055332	3.455116
281.758367	3993.643654	16.773210	-0.055323	3.451856
281.857108	3985.617307	16.778215	-0.055336	3.448583
281.763657	3977.636043	16.783219	-0.055314	3.445320
281.595898	3969.665286	16.788224	-0.055278	3.442055
281.587926	3961.671051	16.793229	-0.055271	3.438783
281.720421	3953.671607	16.798234	-0.055291	3.435510
281.553026	3945.649127	16.803239	-0.055254	3.432215
281.484197	3937.684244	16.808243	-0.055236	3.428943
281.484963	3929.656041	16.813248	-0.055231	3.425645
281.398427	3921.682882	16.818253	-0.055210	3.422363
281.199627	3913.718221	16.823258	-0.055168	3.419078
281.420330	3905.704347	16.828263	-0.055204	3.415783
281.536241	3897.720300	16.833267	-0.055221	3.412494
281.155541	3889.719631	16.838272	-0.055145	3.409178
281.366683	3881.713004	16.843277	-0.055179	3.405877
281.359336	3873.787123	16.848282	-0.055172	3.402598
280.943095	3865.798663	16.853287	-0.055090	3.399276
281.054939	3857.861070	16.858291	-0.055106	3.395990
280.951997	3849.732311	16.863296	-0.055081	3.392614
280.885802	3841.725862	16.868301	-0.055064	3.389287
280.723045	3833.770644	16.873306	-0.055028	3.385975
280.694668	3825.760314	16.878311	-0.055018	3.382641
280.785857	3817.788340	16.883315	-0.055030	3.379324
280.662150	3809.836211	16.888320	-0.055002	3.376004
280.702908	3801.819054	16.893325	-0.055004	3.372660
280.722480	3793.807139	16.898330	-0.055003	3.369314
280.705886	3785.828624	16.903335	-0.054995	3.365977
280.653957	3777.863264	16.908339	-0.054980	3.362641
280.513152	3769.870936	16.913344	-0.054948	3.359287
280.524822	3761.908646	16.918349	-0.054946	3.355948
280.377993	3753.878613	16.923354	-0.054913	3.352572
280.394879	3745.833088	16.928359	-0.054911	3.349191
280.390155	3737.868744	16.933363	-0.054905	3.345841
280.365460	3729.891870	16.938368	-0.054895	3.342481
280.248074	3721.922872	16.943373	-0.054869	3.339118
280.374785	3713.914272	16.948378	-0.054887	3.335743
280.274136	3705.916396	16.953383	-0.054863	3.332361
280.214144	3697.926856	16.958387	-0.054847	3.328981
279.945967	3689.940698	16.963392	-0.054792	3.325591
279.903841	3681.981428	16.968397	-0.054779	3.322218
279.891917	3674.001143	16.973402	-0.054772	3.318833
279.772560	3666.003861	16.978407	-0.054744	3.315433
280.012171	3657.969419	16.983411	-0.054784	3.312028
279.934087	3649.946841	16.988416	-0.054764	3.308612
279.830113	3641.978101	16.993421	-0.054740	3.305215
279.689769	3634.033995	16.998426	-0.054708	3.301823
279.600762	3626.018264	17.003431	-0.054687	3.298399
279.563116	3618.058943	17.008435	-0.054675	3.294998
279.602249	3610.041935	17.013440	-0.054677	3.291571
279.521928	3602.044627	17.018445	-0.054657	3.288144
279.379635	3594.080887	17.023450	-0.054625	3.284726
279.319918	3586.117398	17.028455	-0.054609	3.281308
279.400567	3578.110418	17.033459	-0.054619	3.277873
279.258832	3570.107091	17.038464	-0.054587	3.274427
279.181209	3562.094888	17.043469	-0.054568	3.270977
279.236974	3554.124059	17.048474	-0.054573	3.267545
279.146048	3546.124912	17.053479	-0.054551	3.264092
279.066438	3538.171563	17.058483	-0.054531	3.260656
279.205447	3530.159856	17.063488	-0.054552	3.257199
279.160396	3522.160354	17.068493	-0.054539	3.253737
278.941184	3514.174465	17.073498	-0.054493	3.250270
278.759594	3506.188012	17.078503	-0.054454	3.246800
278.895467	3498.204123	17.083507	-0.054474	3.243341
278.762411	3490.221050	17.088512	-0.054444	3.239867
278.920277	3482.248550	17.093517	-0.054468	3.236406
278.786642	3474.213900	17.098522	-0.054438	3.232903
278.560502	3466.208743	17.103527	-0.054391	3.229405
278.723772	3458.204224	17.108531	-0.054416	3.225919
278.571310	3450.233992	17.113536	-0.054383	3.222431
278.524220	3442.263387	17.118541	-0.054369	3.218944
278.483564	3434.288016	17.123546	-0.054356	3.215451
278.352553	3426.267110	17.128551	-0.054327	3.211930
278.186712	3418.317355	17.133555	-0.054291	3.208436
278.264494	3410.290994	17.138560	-0.054300	3.204914
278.145899	3402.352894	17.143565	-0.054273	3.201419
278.127451	3394.365187	17.148570	-0.054265	3.197902
278.046360	3386.348283	17.153575	-0.054244	3.194366
278.193509	3378.331462	17.158579	-0.054267	3.190836
278.038901	3370.368269	17.163584	-0.054233	3.187313
277.931080	3362.383408	17.168589	-0.054208	3.183778
277.987774	3354.401697	17.173594	-0.054213	3.180248
277.718384	3346.425388	17.178599	-0.054158	3.176702
277.702647	3338.456413	17.183603	-0.054150	3.173166
277.632514	3330.415114	17.188608	-0.054132	3.169592
277.587213	3322.442302	17.193613	-0.054118	3.166046
277.683449	3314.457843	17.198618	-0.054131	3.162496
277.560338	3306.470505	17.203623	-0.054103	3.158932
277.590117	3298.506178	17.208627	-0.054103	3.155380
277.348622	3290.509253	17.213632	-0.054053	3.151798
277.318653	3282.512224	17.218637	-0.054043	3.148221
277.413200	3274.494096	17.223642	-0.054055	3.144636
277.273882	3266.541226	17.228647	-0.054024	3.141066
277.238108	3258.578341	17.233651	-0.054012	3.137492
277.162691	3250.572151	17.238656	-0.053993	3.133893
277.239478	3242.553374	17.243661	-0.054002	3.130290
277.277214	3234.591283	17.248666	-0.054004	3.126708
277.017853	3226.586481	17.253671	-0.053951	3.123088
277.337295	3218.603286	17.258675	-0.054005	3.119500
277.091262	3210.653098	17.263680	-0.053954	3.115898
276.984202	3202.660559	17.268685	-0.053929	3.112278
277.011155	3194.657908	17.273690	-0.053929	3.108655
276.991163	3186.639635	17.278695	-0.053921	3.105020
276.920015	3178.716282	17.283699	-0.053902	3.101420
276.840171	3170.717199	17.288704	-0.053882	3.097782
276.825308	3162.708043	17.293709	-0.053874	3.094138
276.713407	3154.713923	17.298714	-0.053848	3.090491
276.649689	3146.740891	17.303719	-0.053831	3.086853
276.726475	3138.774815	17.308723	-0.053841	3.083219
276.675240	3130.775671	17.313728	-0.053826	3.079561
276.576994	3122.809888	17.318733	-0.053803	3.075911
276.658393	3114.753083	17.323738	-0.053813	3.072223
276.711565	3106.722369	17.328743	-0.053817	3.068541
276.334080	3098.791096	17.333747	-0.053742	3.064881
276.350844	3090.810473	17.338752	-0.053740	3.061212
276.575635	3082.826385	17.343757	-0.053777	3.057547
276.328400	3074.852476	17.348762	-0.053726	3.053860
276.369211	3066.835254	17.353767	-0.053728	3.050162
276.292117	3058.903946	17.358771	-0.053709	3.046494
275.916934	3050.951408	17.363776	-0.053634	3.042797
275.989731	3042.949932	17.368781	-0.053642	3.039094
276.023766	3034.974942	17.373786	-0.053644	3.035397
276.108411	3026.933878	17.378791	-0.053654	3.031668
276.017351	3018.973161	17.383795	-0.053632	3.027963
275.974132	3010.974387	17.388800	-0.053619	3.024237
275.831057	3003.024630	17.393805	-0.053587	3.020526
275.836097	2995.062653	17.398810	-0.053583	3.016811
275.691272	2987.051276	17.403815	-0.053551	3.013061
275.742552	2979.029507	17.408819	-0.053556	3.009311
275.505969	2971.066428	17.413824	-0.053506	3.005570
275.518965	2963.121872	17.418829	-0.053504	3.001845
275.535233	2955.155596	17.423834	-0.053502	2.998106
275.429695	2947.139704	17.428839	-0.053477	2.994332
275.257719	2939.146265	17.433843	-0.053440	2.990561
275.178333	2931.158537	17.438848	-0.053420	2.986792
275.260742	2923.142690	17.443853	-0.053430	2.983014
275.284651	2915.186728	17.448858	-0.053430	2.979256
275.091579	2907.224881	17.453863	-0.053389	2.975480
275.126858	2899.231213	17.458867	-0.053390	2.971695
275.094610	2891.226609	17.463872	-0.053379	2.967897
275.149866	2883.243968	17.468877	-0.053384	2.964108
275.245250	2875.271156	17.473882	-0.053397	2.960322
275.002517	2867.306000	17.478887	-0.053346	2.956517
274.956050	2859.314488	17.483891	-0.053333	2.952705
274.839596	2851.333647	17.488896	-0.053306	2.948889
275.003258	2843.306962	17.493901	-0.053331	2.945061
274.890116	2835.390204	17.498906	-0.053305	2.941266
274.569516	2827.419527	17.503911	-0.053240	2.937430
274.772337	2819.417140	17.508915	-0.053273	2.933600
274.712397	2811.397716	17.513920	-0.053257	2.929744
274.594582	2803.446393	17.518925	-0.053230	2.925912
274.550659	2795.491688	17.523930	-0.053217	2.922078
274.597702	2787.505201	17.528935	-0.053220	2.918228
274.432205	2779.516894	17.533939	-0.053184	2.914361
274.325479	2771.443838	17.538944	-0.053159	2.910450
274.341692	2763.470653	17.543949	-0.053157	2.906590
274.371418	2755.514292	17.548954	-0.053158	2.902733
274.322018	2747.537350	17.553959	-0.053143	2.898857
274.433810	2739.562344	17.558963	-0.053159	2.894985
274.371385	2731.571666	17.563968	-0.053142	2.891091
274.153598	2723.627506	17.568973	-0.053097	2.887206
274.191655	2715.648591	17.573978	-0.053099	2.883312
274.131089	2707.665839	17.578983	-0.053082	2.879406
274.011698	2699.708132	17.583987	-0.053055	2.875504
273.984514	2691.701393	17.588992	-0.053045	2.871577
273.985483	2683.697398	17.593997	-0.053040	2.867648
274.018033	2675.742735	17.599002	-0.053041	2.863740
273.816747	2667.762317	17.604007	-0.052998	2.859801
273.963575	2659.791984	17.609011	-0.053021	2.855880
273.719351	2651.826465	17.614016	-0.052970	2.851935
273.397633	2643.853042	17.619021	-0.052905	2.847976
273.550001	2635.857034	17.624026	-0.052928	2.844026
273.558530	2627.871280	17.629031	-0.052925	2.840069
273.551758	2619.923524	17.634035	-0.052919	2.836123
273.418048	2611.910187	17.639040	-0.052889	2.832133
273.389731	2603.920084	17.644045	-0.052878	2.828154
273.365182	2595.953956	17.649050	-0.052868	2.824182
273.376181	2587.958753	17.654055	-0.052865	2.820192
273.396795	2580.000601	17.659059	-0.052864	2.816215
273.401191	2572.013148	17.664064	-0.052860	2.812217
273.046493	2564.046377	17.669069	-0.052789	2.808203
272.934273	2556.075844	17.674074	-0.052763	2.804195
272.853975	2548.109381	17.679079	-0.052743	2.800186
273.016617	2540.141939	17.684083	-0.052768	2.796184
272.805627	2532.134776	17.689088	-0.052724	2.792135
272.762934	2524.150211	17.694093	-0.052711	2.788101
272.788866	2516.162509	17.699098	-0.052710	2.784063
272.721077	2508.184902	17.704103	-0.052693	2.780020
272.711879	2500.249059	17.709107	-0.052686	2.775995
272.630103	2492.263126	17.714112	-0.052665	2.771934
272.703317	2484.246991	17.719117	-0.052674	2.767862
272.754367	2476.291131	17.724122	-0.052678	2.763812
272.543516	2468.334039	17.729127	-0.052634	2.759741
272.551211	2460.391962	17.734131	-0.052630	2.755684
272.329728	2452.306085	17.739136	-0.052584	2.751534
272.512011	2444.311211	17.744141	-0.052613	2.747449
272.455014	2436.364135	17.749146	-0.052597	2.743367
272.080803	2428.418286	17.754151	-0.052522	2.739261
272.151358	2420.450930	17.759155	-0.052530	2.735165
272.156242	2412.451171	17.764160	-0.052526	2.731042
272.087201	2404.479483	17.769165	-0.052508	2.726922
271.939521	2396.527985	17.774170	-0.052476	2.722802
271.876205	2388.567149	17.779175	-0.052459	2.718676
271.893340	2380.607668	17.784179	-0.052457	2.714549
271.816049	2372.590433	17.789184	-0.052438	2.710381
271.838646	2364.604850	17.794189	-0.052437	2.706228
271.847733	2356.661864	17.799194	-0.052433	2.702090
271.611030	2348.710813	17.804199	-0.052384	2.697927
271.703009	2340.722643	17.809203	-0.052396	2.693758
271.643120	2332.718518	17.814208	-0.052380	2.689565
271.601165	2324.755101	17.819213	-0.052367	2.685388
271.524847	2316.826653	17.824218	-0.052348	2.681220
271.500571	2308.849720	17.829223	-0.052338	2.677024
271.320384	2300.866822	17.834227	-0.052299	2.672808
271.082003	2292.885921	17.839232	-0.052250	2.668583
271.141916	2284.875157	17.844237	-0.052256	2.664354
271.191727	2276.928994	17.849242	-0.052260	2.660152
270.874408	2268.978773	17.854247	-0.052196	2.655918
271.086950	2260.961035	17.859251	-0.052231	2.651675
271.041230	2252.988084	17.864256	-0.052217	2.647432
271.070800	2245.031333	17.869261	-0.052217	2.643197
270.777582	2237.111599	17.874266	-0.052158	2.638953
270.989386	2229.095313	17.879271	-0.052192	2.634683
270.843775	2221.129051	17.884275	-0.052160	2.630410
270.780497	2213.149983	17.889280	-0.052143	2.626129
270.559462	2205.205707	17.894285	-0.052097	2.621849
270.663759	2197.246304	17.899290	-0.052111	2.617575
270.422955	2189.268913	17.904295	-0.052061	2.613262
270.431003	2181.271159	17.909299	-0.052058	2.608947
270.347428	2173.320199	17.914304	-0.052037	2.604644
270.390067	2165.349476	17.919309	-0.052040	2.600332
270.374290	2157.414449	17.924314	-0.052032	2.596028
270.115065	2149.281120	17.929319	-0.051978	2.591592
270.242934	2141.278427	17.934323	-0.051997	2.587247
270.116910	2133.352279	17.939328	-0.051968	2.582918
269.962026	2125.423100	17.944333	-0.051935	2.578579
270.221238	2117.447219	17.949338	-0.051978	2.574235
270.167571	2109.461821	17.954343	-0.051963	2.569857
270.019104	2101.548014	17.959347	-0.051930	2.565504
270.040769	2093.596804	17.964352	-0.051929	2.561135
270.001420	2085.645021	17.969357	-0.051917	2.556754
269.913513	2077.674275	17.974362	-0.051895	2.552352
269.816535	2069.682906	17.979367	-0.051872	2.547930
269.812917	2061.739578	17.984371	-0.051866	2.543533
269.849264	2053.770030	17.989376	-0.051868	2.539117
269.704667	2045.813428	17.994381	-0.051836	2.534688
269.662711	2037.842904	17.999386	-0.051823	2.530251
269.428690	2029.888742	18.004391	-0.051774	2.525801
269.522994	2021.925004	18.009395	-0.051787	2.521361
269.498127	2013.967312	18.014400	-0.051777	2.516909
269.282769	2005.973212	18.019405	-0.051732	2.512414
269.507350	1997.974114	18.024410	-0.051769	2.507940
269.433486	1990.010533	18.029415	-0.051750	2.503457
269.414751	1982.059984	18.034419	-0.051741	2.498977
269.127879	1974.138322	18.039424	-0.051683	2.494486
269.128313	1966.137502	18.044429	-0.051678	2.489962
269.081915	1958.193608	18.049434	-0.051664	2.485460
268.997861	1950.229972	18.054439	-0.051643	2.480935
268.987803	1942.292726	18.059443	-0.051636	2.476422
268.832548	1934.319771	18.064448	-0.051602	2.471870
268.713481	1926.344318	18.069453	-0.051575	2.467311
268.825159	1918.379300	18.074458	-0.051591	2.462766
268.636516	1910.432090	18.079463	-0.051551	2.458201
268.727325	1902.448882	18.084467	-0.051562	2.453628
268.635977	1894.488290	18.089472	-0.051540	2.449045
268.516679	1886.534121	18.094477	-0.051513	2.444455
268.532626	1878.584529	18.099482	-0.051511	2.439870
268.435761	1870.628251	18.104487	-0.051488	2.435263
268.416628	1862.581809	18.109491	-0.051479	2.430602
268.290317	1854.640170	18.114496	-0.051451	2.425984
268.439678	1846.650015	18.119501	-0.051473	2.421350
268.286871	1838.748418	18.124506	-0.051440	2.416736
268.156817	1830.783637	18.129511	-0.051410	2.412077
267.986259	1822.833815	18.134515	-0.051374	2.407416
267.952963	1814.874100	18.139520	-0.051362	2.402750
267.997009	1806.913211	18.144525	-0.051365	2.398080
268.077939	1798.953075	18.149530	-0.051375	2.393404
267.782385	1790.982107	18.154535	-0.051315	2.388684
267.768696	1783.034374	18.159539	-0.051308	2.383990
267.689669	1775.093890	18.164544	-0.051288	2.379285
267.533848	1767.148124	18.169549	-0.051254	2.374563
267.672932	1759.159842	18.174554	-0.051275	2.369828
267.457309	1751.218772	18.179559	-0.051229	2.365085
267.508740	1743.281152	18.184563	-0.051234	2.360355
267.666535	1735.306464	18.189568	-0.051258	2.355602
267.238766	1727.355575	18.194573	-0.051174	2.350806
267.369117	1719.377307	18.199578	-0.051193	2.346030
267.397133	1711.400493	18.204583	-0.051193	2.341236
267.332883	1703.482239	18.209587	-0.051176	2.336460
267.383919	1695.500266	18.214592	-0.051180	2.331645
267.272890	1687.556217	18.219597	-0.051154	2.326830
267.110633	1679.630235	18.224602	-0.051119	2.322012
267.011856	1671.688547	18.229607	-0.051096	2.317179
267.083545	1663.719240	18.234611	-0.051104	2.312334
267.126674	1655.735713	18.239616	-0.051107	2.307467
266.727083	1647.833079	18.244621	-0.051028	2.302602
266.871746	1639.867553	18.249626	-0.051049	2.297735
266.758118	1631.910265	18.254631	-0.051023	2.292840
266.577012	1623.972708	18.259635	-0.050984	2.287941
266.598786	1616.020325	18.264640	-0.050983	2.283039
266.627689	1608.066850	18.269645	-0.050984	2.278127
266.506478	1600.120219	18.274650	-0.050956	2.273196
266.299703	1592.106482	18.279655	-0.050912	2.268205
266.598899	1584.114268	18.284659	-0.050963	2.263260
266.578441	1576.184308	18.289664	-0.050954	2.258316
266.310135	1568.265141	18.294669	-0.050899	2.253345
266.259757	1560.328133	18.299674	-0.050885	2.248372
266.507159	1552.328293	18.304679	-0.050926	2.243374
266.315161	1544.441485	18.309683	-0.050885	2.238397
266.156184	1536.513799	18.314688	-0.050850	2.233387
266.096929	1528.530838	18.319693	-0.050834	2.228339
266.076407	1520.596534	18.324698	-0.050825	2.223314
265.806286	1512.687098	18.329703	-0.050770	2.218271
265.795886	1504.742744	18.334707	-0.050763	2.213217
265.748888	1496.783262	18.339712	-0.050749	2.208139
265.673780	1488.838251	18.344717	-0.050730	2.203056
265.622196	1480.923883	18.349722	-0.050715	2.197983
265.494680	1472.952526	18.354727	-0.050686	2.192854
265.328508	1464.992262	18.359731	-0.050650	2.187718
265.412429	1457.038412	18.364736	-0.050661	2.182596
265.380359	1449.102691	18.369741	-0.050650	2.177463
265.285976	1441.170939	18.374746	-0.050627	2.172315
265.258209	1433.195776	18.379751	-0.050617	2.167132
265.277971	1425.279395	18.384755	-0.050616	2.161980
265.244468	1417.356226	18.389760	-0.050604	2.156806
265.164737	1409.400036	18.394765	-0.050584	2.151594
265.109359	1401.461830	18.399770	-0.050569	2.146383
265.105153	1393.514267	18.404775	-0.050563	2.141158
264.939091	1385.597418	18.409779	-0.050527	2.135925
264.777815	1377.660448	18.414784	-0.050492	2.130666
264.743427	1369.713430	18.419789	-0.050481	2.125400
264.849273	1361.790390	18.424794	-0.050495	2.120150
264.572072	1353.875222	18.429799	-0.050439	2.114856
264.536398	1345.861385	18.434803	-0.050427	2.109505
264.677721	1337.907144	18.439808	-0.050448	2.104198
264.707080	1329.973208	18.444813	-0.050449	2.098880
264.546217	1322.075720	18.449818	-0.050414	2.093555
264.357976	1314.140636	18.454823	-0.050373	2.088188
264.389117	1306.206714	18.459827	-0.050374	2.082830
264.323347	1298.295962	18.464832	-0.050357	2.077464
264.374793	1290.338830	18.469837	-0.050361	2.072064
264.480570	1282.390805	18.474842	-0.050376	2.066661
264.209680	1274.483904	18.479847	-0.050321	2.061235
264.165210	1266.572922	18.484851	-0.050307	2.055815
264.046647	1258.625745	18.489856	-0.050280	2.050348
263.968256	1250.705730	18.494861	-0.050260	2.044888
263.991395	1242.797442	18.499866	-0.050260	2.039433
263.700475	1234.887204	18.504871	-0.050201	2.033930
263.784756	1226.905246	18.509875	-0.050211	2.028400
263.701123	1218.986029	18.514880	-0.050190	2.022881
263.605749	1211.067848	18.519885	-0.050168	2.017347
263.714066	1203.134929	18.524890	-0.050183	2.011809
263.585186	1195.193680	18.529895	-0.050154	2.006224
263.458805	1187.301946	18.534899	-0.050125	2.000660
263.540653	1179.379082	18.539904	-0.050135	1.995079
263.340638	1171.439892	18.544909	-0.050093	1.989442
263.394330	1163.522355	18.549914	-0.050098	1.983830
263.204553	1155.622161	18.554919	-0.050058	1.978190
263.034775	1147.711718	18.559923	-0.050021	1.972528
263.019813	1139.783153	18.564928	-0.050013	1.966853
262.958323	1131.854860	18.569933	-0.049997	1.961157
262.888643	1123.968387	18.574938	-0.049979	1.955473
262.753200	1115.993786	18.579943	-0.049948	1.949702
262.924381	1108.041707	18.584947	-0.049975	1.943964
262.917740	1100.138760	18.589952	-0.049969	1.938225
262.671232	1092.249217	18.594957	-0.049918	1.932452
262.741804	1084.314597	18.599962	-0.049926	1.926664
262.659446	1076.405065	18.604967	-0.049906	1.920860
262.807357	1068.484958	18.609971	-0.049928	1.915056
262.717772	1060.574242	18.614976	-0.049906	1.909216
262.498043	1052.676048	18.619981	-0.049860	1.903351
262.734482	1044.754717	18.624986	-0.049899	1.897503
262.517295	1036.848825	18.629991	-0.049854	1.891597
262.383376	1028.955344	18.634995	-0.049824	1.885691
262.253752	1021.084354	18.640000	-0.049795	1.879784
261.890793	1013.217240	18.645005	-0.049722	1.873834
262.091254	1005.238242	18.650010	-0.049754	1.867846
262.101709	997.308451	18.655015	-0.049751	1.861854
261.810706	989.452040	18.660019	-0.049692	1.855863
261.674470	981.546735	18.665024	-0.049662	1.849833
261.503613	973.652578	18.670029	-0.049625	1.843789
261.592047	965.749140	18.675034	-0.049636	1.837747
261.492664	957.838537	18.680039	-0.049613	1.831658
261.621506	949.902424	18.685043	-0.049632	1.825556
261.604877	942.023540	18.690048	-0.049623	1.819461
261.441148	934.136466	18.695053	-0.049588	1.813321
261.478771	926.228932	18.700058	-0.049590	1.807168
261.297114	918.359188	18.705063	-0.049551	1.800998
261.150248	910.496844	18.710067	-0.049519	1.794816
261.078495	902.536546	18.715072	-0.049500	1.788545
261.169974	894.616378	18.720077	-0.049512	1.782304
261.277383	886.725873	18.725082	-0.049527	1.776066
261.018806	878.856528	18.730087	-0.049474	1.769777
260.993538	870.975910	18.735091	-0.049464	1.763487
260.876351	863.114749	18.740096	-0.049437	1.757177
260.758582	855.217796	18.745101	-0.049411	1.750816
260.652594	847.352979	18.750106	-0.049386	1.744460
260.477447	839.479384	18.755111	-0.049348	1.738064
260.568633	831.568250	18.760115	-0.049360	1.731648
260.749649	823.658074	18.765120	-0.049389	1.725220
260.359562	815.854431	18.770125	-0.049311	1.718782
260.653133	807.927387	18.775130	-0.049361	1.712307
260.514209	800.034010	18.780135	-0.049330	1.705778
260.190051	792.226461	18.785139	-0.049264	1.699272
260.170214	784.343710	18.790144	-0.049256	1.692718
260.038033	776.454860	18.795149	-0.049226	1.686118
259.973171	768.606596	18.800154	-0.049209	1.679536
259.988464	760.724358	18.805159	-0.049207	1.672909
260.015365	752.826597	18.810163	-0.049207	1.666245
260.042991	744.968498	18.815168	-0.049207	1.659587
259.856900	737.122901	18.820173	-0.049167	1.652885
259.813698	729.253891	18.825178	-0.049154	1.646154
259.705554	721.413954	18.830183	-0.049129	1.639413
259.622158	713.546500	18.835187	-0.049109	1.632622
259.554187	705.650822	18.840192	-0.049091	1.625781
259.647999	697.775245	18.845197	-0.049103	1.618952
259.434821	689.959196	18.850202	-0.049059	1.612102
259.117662	682.127770	18.855207	-0.048995	1.605195
259.204899	674.274466	18.860211	-0.049006	1.598296
259.425954	666.377372	18.865216	-0.049042	1.591347
259.179931	658.558869	18.870221	-0.048991	1.584371
259.056946	650.744701	18.875226	-0.048963	1.577385
258.959015	642.891090	18.880231	-0.048940	1.570337
258.832071	635.070352	18.885235	-0.048911	1.563282
258.816660	627.240247	18.890240	-0.048904	1.556203
258.578757	619.399876	18.895245	-0.048854	1.549050
258.668473	611.549333	18.900250	-0.048866	1.541902
258.513599	603.729461	18.905255	-0.048832	1.534713
258.413695	595.892911	18.910259	-0.048808	1.527483
258.406305	588.069195	18.915264	-0.048802	1.520244
258.318101	580.250745	18.920269	-0.048781	1.512964
258.128741	572.440906	18.925274	-0.048740	1.505640
258.143835	564.607972	18.930279	-0.048738	1.498291
258.056732	556.789434	18.935283	-0.048717	1.490903
258.035266	548.982664	18.940288	-0.048708	1.483500
258.219604	541.141551	18.945293	-0.048737	1.476058
258.161106	533.293751	18.950298	-0.048722	1.468535
257.735838	525.541777	18.955303	-0.048637	1.461007
257.760869	517.736414	18.960307	-0.048637	1.453460
257.758478	509.921528	18.965312	-0.048632	1.445860
257.467322	502.176055	18.970317	-0.048573	1.438241
257.457748	494.362420	18.975322	-0.048566	1.430561
257.595777	486.533520	18.980327	-0.048586	1.422847
257.475213	478.776338	18.985331	-0.048559	1.415121
257.395422	470.986873	18.990336	-0.048539	1.407326
257.279370	463.220513	18.995341	-0.048513	1.399505
257.334290	455.431343	19.000346	-0.048518	1.391646
256.956563	447.688983	19.005351	-0.048443	1.383717
256.951106	439.911851	19.010355	-0.048437	1.375770
257.126772	432.100789	19.015360	-0.048464	1.367772
257.015350	424.351380	19.020365	-0.048439	1.359742
256.829206	416.625646	19.025370	-0.048399	1.351676
256.753127	408.860828	19.030375	-0.048380	1.343539
256.653092	401.121650	19.035379	-0.048356	1.335376
256.433740	393.392731	19.040384	-0.048311	1.327152
256.224952	385.677175	19.045389	-0.048267	1.318893
256.302640	377.834870	19.050394	-0.048276	1.310498
255.993059	370.091473	19.055399	-0.048214	1.302085
255.880140	362.380831	19.060403	-0.048188	1.293688
255.952101	354.632933	19.065408	-0.048196	1.285230
255.733786	346.952061	19.070413	-0.048151	1.276736
255.495957	339.262487	19.075418	-0.048102	1.268172
255.381754	331.559264	19.080423	-0.048075	1.259557
255.276107	323.858877	19.085427	-0.048051	1.250888
254.743479	316.241235	19.090432	-0.047947	1.242171
254.640730	308.536418	19.095437	-0.047923	1.233375
254.269186	300.876512	19.100442	-0.047849	1.224515
253.907323	293.220319	19.105447	-0.047776	1.215596
253.557829	285.562808	19.110451	-0.047706	1.206612
253.246006	277.928693	19.115456	-0.047644	1.197596
252.656255	270.306463	19.120461	-0.047529	1.188469
252.520708	262.638427	19.125466	-0.047499	1.179310
252.067043	255.020581	19.130471	-0.047409	1.170073
251.791007	247.386294	19.135475	-0.047353	1.160779
251.383179	239.763446	19.140480	-0.047272	1.151397
250.788106	232.164833	19.145485	-0.047157	1.141928
250.600465	224.537634	19.150490	-0.047117	1.132431
250.093308	216.955535	19.155495	-0.047018	1.122841
249.803014	209.360561	19.160499	-0.046959	1.113199
249.400355	201.780532	19.165504	-0.046879	1.103467
249.029176	194.210889	19.170509	-0.046805	1.093669
248.623859	186.656811	19.175514	-0.046725	1.083795
248.189895	179.113619	19.180519	-0.046639	1.073837
247.783469	171.561848	19.185523	-0.046559	1.063781
247.311821	164.044471	19.190528	-0.046466	1.053660
246.699206	156.547451	19.195533	-0.046347	1.043434
246.459611	149.018316	19.200538	-0.046298	1.033152
245.971136	141.517642	19.205543	-0.046202	1.022746
245.623612	134.023695	19.210547	-0.046133	1.012276
245.425561	126.518651	19.215552	-0.046091	1.001717
245.010942	119.047327	19.220557	-0.046009	0.991040
244.539597	111.592983	19.225562	-0.045916	0.980257
244.047609	104.167998	19.230567	-0.045820	0.969391
243.474747	96.780461	19.235571	-0.045709	0.958436
243.185915	89.344032	19.240576	-0.045650	0.947355
242.652742	81.979439	19.245581	-0.045546	0.936187
242.326370	74.594795	19.250586	-0.045481	0.924908
241.777164	67.267241	19.255591	-0.045374	0.913517
241.122881	60.185624	19.260595	-0.045247	0.902338