Tue Mar 23 11:40:07 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.880129	0.017228	0.000000	0.000015	0.722378

0.705985	0.082923	0.005005	0.000047	0.722447
0.747903	0.105864	0.010010	0.000039	0.722507
0.746215	0.039083	0.015014	0.000040	0.722375
0.796507	0.029256	0.020019	0.000030	0.722373
0.863262	0.021188	0.025024	0.000018	0.722381
0.948752	0.002155	0.030029	0.000002	0.722374
0.908221	0.012908	0.035034	0.000009	0.722381
0.813795	0.026102	0.040038	0.000027	0.722374
0.909753	0.009219	0.045043	0.000009	0.722374
0.887878	0.015578	0.050048	0.000013	0.722379
0.681750	0.048102	0.055053	0.000051	0.722371
0.813824	0.029041	0.060058	0.000026	0.722380
0.796597	0.028373	0.065062	0.000029	0.722373
0.885562	0.012854	0.070067	0.000013	0.722374
0.983646	-0.000593	0.075072	-0.000006	0.722382
0.993367	-0.051595	0.080077	-0.000008	0.722285
0.805052	-0.121240	0.085082	0.000028	0.722083
0.848718	-0.131754	0.090086	0.000019	0.722078
0.764619	-0.117973	0.095091	0.000035	0.722075
1.103693	-0.174721	0.100096	-0.000028	0.722083
0.677652	-0.100622	0.105101	0.000051	0.722079
0.772543	-0.114178	0.110106	0.000033	0.722086
0.785422	-0.249631	0.115110	0.000031	0.721824
0.703932	-0.273994	0.120115	0.000046	0.721748
0.817231	-0.292179	0.125120	0.000025	0.721752
0.849005	-0.302123	0.130125	0.000019	0.721744
0.842722	-0.294889	0.135130	0.000020	0.721756
0.743371	-0.397879	0.140134	0.000038	0.721519
0.958580	-0.474413	0.145139	-0.000002	0.721444
1.027151	-0.483882	0.150144	-0.000015	0.721450
0.558632	-0.406064	0.155149	0.000072	0.721439
0.736396	-0.518701	0.160154	0.000039	0.721280
0.895131	-0.624244	0.165158	0.000010	0.721128
0.866819	-0.620274	0.170163	0.000015	0.721126
0.783465	-0.603251	0.175168	0.000030	0.721130
0.691822	-0.694540	0.180173	0.000047	0.720919
0.866185	-0.740494	0.185178	0.000015	0.720889
0.681881	-0.711130	0.190182	0.000049	0.720883
0.617811	-0.776130	0.195187	0.000061	0.720733
0.866288	-0.914201	0.200192	0.000015	0.720548
0.721955	-0.891753	0.205197	0.000042	0.720542
0.694258	-0.931687	0.210202	0.000047	0.720454
0.693302	-1.045716	0.215206	0.000047	0.720229
0.519699	-1.015083	0.220211	0.000079	0.720228
0.564996	-1.076867	0.225216	0.000071	0.720123
0.470102	-1.171266	0.230221	0.000088	0.719904
0.496251	-1.175011	0.235226	0.000083	0.719905
0.293593	-1.215942	0.240230	0.000121	0.719754
0.480522	-1.327650	0.245235	0.000086	0.719599
0.535409	-1.331881	0.250240	0.000076	0.719610
0.407811	-1.452865	0.255245	0.000100	0.719327
0.634267	-1.516810	0.260250	0.000057	0.719281
0.509875	-1.547161	0.265254	0.000080	0.719177
0.168727	-1.594835	0.270259	0.000144	0.718964
-0.044528	-1.552551	0.275264	0.000184	0.718972
-0.050943	-1.682055	0.280269	0.000185	0.718715
0.137826	-1.746465	0.285274	0.000150	0.718654
0.234299	-1.818866	0.290278	0.000132	0.718545
0.132617	-1.895728	0.295283	0.000150	0.718358
-0.099789	-1.852564	0.300288	0.000194	0.718361
-0.328952	-1.985622	0.305293	0.000236	0.718018
-0.420115	-1.966109	0.310298	0.000253	0.718025
-0.661646	-2.025577	0.315302	0.000298	0.717822
-0.813437	-2.058006	0.320307	0.000326	0.717705
-0.368528	-2.175607	0.325312	0.000243	0.717629
-1.747799	-2.054937	0.330317	0.000500	0.717382
-1.892719	-2.026721	0.335322	0.000527	0.717387
-1.770272	-2.139827	0.340326	0.000504	0.717207
-2.888892	-2.002033	0.345331	0.000712	0.717085
-2.673999	-2.039001	0.350336	0.000672	0.717088
-2.994771	-2.093481	0.355341	0.000732	0.716867
-3.790496	-2.004680	0.360346	0.000880	0.716763
-3.598287	-2.041789	0.365350	0.000844	0.716757
-3.752915	-2.062581	0.370355	0.000873	0.716662
-4.596174	-2.016726	0.375360	0.001030	0.716455
-4.233425	-2.085231	0.380365	0.000962	0.716448
-4.567871	-2.023185	0.385370	0.001024	0.716453
-4.677845	-2.121444	0.390374	0.001045	0.716219
-5.625718	-1.997808	0.395379	0.001221	0.716130
-5.517865	-2.011936	0.400384	0.001201	0.716140
-5.383481	-2.040045	0.405389	0.001176	0.716132
-5.525648	-2.091917	0.410394	0.001202	0.715979
-6.510269	-1.963174	0.415398	0.001385	0.715887
-6.198065	-2.019763	0.420403	0.001327	0.715885
-5.862984	-2.075505	0.425408	0.001265	0.715893
-6.546416	-1.997053	0.430413	0.001392	0.715808
-7.192890	-2.009916	0.435418	0.001512	0.715554
-6.755942	-2.089432	0.440422	0.001431	0.715551
-7.482274	-1.963175	0.445427	0.001566	0.715545
-7.294722	-1.990795	0.450432	0.001531	0.715556
-7.127138	-2.051535	0.455437	0.001500	0.715495
-7.999504	-2.024261	0.460442	0.001662	0.715241
-7.972237	-2.031950	0.465446	0.001657	0.715236
-8.350551	-1.964725	0.470451	0.001727	0.715236
-7.951543	-2.033276	0.475456	0.001653	0.715241
-7.813971	-2.063522	0.480461	0.001627	0.715229
-8.647730	-2.061828	0.485466	0.001782	0.714938
-9.070944	-1.999304	0.490470	0.001861	0.714913
-9.181841	-1.979709	0.495475	0.001882	0.714913
-8.944901	-2.020811	0.500480	0.001837	0.714915
-8.976505	-2.019114	0.505485	0.001843	0.714907
-8.705761	-2.075634	0.510490	0.001793	0.714891
-9.523688	-2.070356	0.515494	0.001945	0.714613
-9.773051	-2.028180	0.520499	0.001991	0.714608
-9.842903	-2.013026	0.525504	0.002004	0.714614
-9.944858	-1.998796	0.530509	0.002023	0.714606
-10.161778	-1.955285	0.535514	0.002063	0.714616
-9.789193	-2.021532	0.540518	0.001994	0.714616
-9.975923	-2.146657	0.545523	0.002029	0.714302
-10.875272	-1.996007	0.550528	0.002196	0.714283
-11.220768	-1.938394	0.555533	0.002260	0.714275
-10.548374	-2.053764	0.560538	0.002135	0.714284
-10.592489	-2.046339	0.565542	0.002143	0.714284
-11.153119	-1.949502	0.570547	0.002247	0.714278
-10.507069	-2.135317	0.575552	0.002127	0.714137
-11.730497	-2.001072	0.580557	0.002355	0.713971
-11.497529	-2.039390	0.585562	0.002311	0.713978
-11.329817	-2.071110	0.590566	0.002280	0.713974
-11.666899	-2.012794	0.595571	0.002343	0.713971
-11.508382	-2.036555	0.600576	0.002313	0.713980
-11.671531	-2.036862	0.605581	0.002343	0.713922
-12.238035	-2.069371	0.610586	0.002449	0.713657
-12.236682	-2.071417	0.615590	0.002448	0.713653
-13.024582	-1.931656	0.620595	0.002595	0.713652
-12.369037	-2.044152	0.625600	0.002473	0.713661
-12.394796	-2.046275	0.630605	0.002478	0.713648
-12.944509	-1.942506	0.635610	0.002580	0.713659
-12.645926	-2.034230	0.640614	0.002524	0.713583
-13.331643	-2.024369	0.645619	0.002652	0.713360
-13.242516	-2.035774	0.650624	0.002635	0.713369
-13.779554	-1.945562	0.655629	0.002735	0.713358
-13.444541	-2.002180	0.660634	0.002673	0.713364
-13.298515	-2.029291	0.665638	0.002645	0.713362
-13.685109	-1.960622	0.670643	0.002717	0.713362
-13.361991	-2.053563	0.675648	0.002657	0.713292
-14.268940	-2.026787	0.680653	0.002826	0.713024
-14.224310	-2.032072	0.685658	0.002817	0.713029
-14.670025	-1.952751	0.690662	0.002900	0.713029
-14.243339	-2.029349	0.695667	0.002821	0.713028
-13.977469	-2.072516	0.700672	0.002771	0.713037
-14.402007	-2.002261	0.705677	0.002850	0.713026
-14.279216	-2.071261	0.710682	0.002827	0.712932
-14.884069	-2.070795	0.715686	0.002940	0.712719
-15.155497	-2.024911	0.720691	0.002990	0.712714
-15.311201	-1.992941	0.725696	0.003019	0.712723
-15.320253	-1.997560	0.730701	0.003021	0.712711
-15.269261	-2.002216	0.735706	0.003011	0.712719
-15.230212	-2.009839	0.740710	0.003004	0.712718
-15.339750	-2.036294	0.745715	0.003024	0.712627
-16.082844	-2.019923	0.750720	0.003162	0.712396
-16.337417	-1.980722	0.755725	0.003210	0.712384
-16.121244	-2.015473	0.760730	0.003169	0.712392
-15.871412	-2.059119	0.765734	0.003123	0.712393
-16.230850	-1.997397	0.770739	0.003190	0.712389
-16.160236	-2.004846	0.775744	0.003176	0.712399
-16.211278	-2.010952	0.780749	0.003186	0.712369
-16.732748	-2.055357	0.785754	0.003283	0.712096
-17.223395	-1.969867	0.790758	0.003374	0.712092
-17.270343	-1.962247	0.795763	0.003383	0.712091
-16.867654	-2.028937	0.800768	0.003308	0.712101
-17.336750	-1.951788	0.805773	0.003395	0.712088
-17.301447	-1.953967	0.810778	0.003388	0.712097
-16.890295	-2.026627	0.815782	0.003312	0.712098
-17.380966	-2.056032	0.820787	0.003403	0.711865
-18.267807	-1.945239	0.825792	0.003568	0.711771
-18.114150	-1.978133	0.830797	0.003539	0.711760
-17.892079	-2.013000	0.835802	0.003498	0.711770
-18.189725	-1.960756	0.840806	0.003553	0.711769
-18.044185	-1.988407	0.845811	0.003526	0.711765
-17.900647	-2.012062	0.850816	0.003499	0.711769
-18.351104	-1.963510	0.855821	0.003583	0.711706
-18.699198	-2.024465	0.860826	0.003648	0.711461
-18.226938	-2.110207	0.865830	0.003560	0.711458
-19.142187	-1.950199	0.870835	0.003730	0.711452
-19.154459	-1.944140	0.875840	0.003732	0.711460
-18.699759	-2.028866	0.880845	0.003647	0.711453
-18.765272	-2.012892	0.885850	0.003660	0.711461
-18.565725	-2.103870	0.890854	0.003622	0.711351
-19.798366	-1.988987	0.895859	0.003852	0.711142
-19.165900	-2.098073	0.900864	0.003734	0.711149
-19.607316	-2.024121	0.905869	0.003816	0.711140
-20.023205	-1.946663	0.910874	0.003893	0.711147
-19.561525	-2.029896	0.915878	0.003807	0.711145
-19.868105	-1.977269	0.920883	0.003864	0.711141
-19.656448	-2.075696	0.925888	0.003825	0.711020
-20.315516	-2.030158	0.930893	0.003947	0.710877
-20.391020	-2.015025	0.935898	0.003961	0.710881
-20.502063	-1.995945	0.940902	0.003982	0.710879
-20.482186	-2.004021	0.945907	0.003978	0.710870
-19.965719	-2.090176	0.950912	0.003882	0.710882
-20.515112	-2.004918	0.955917	0.003984	0.710857
-21.440473	-1.998337	0.960922	0.004156	0.710541
-21.069855	-2.064840	0.965926	0.004087	0.710540
-21.643452	-1.965572	0.970931	0.004194	0.710535
-21.445250	-1.996981	0.975936	0.004157	0.710543
-21.501039	-1.992237	0.980941	0.004167	0.710532
-21.448174	-1.996969	0.985946	0.004157	0.710542
-21.397309	-2.007673	0.990950	0.004148	0.710539
-22.063262	-2.024196	0.995955	0.004272	0.710269
-22.277908	-2.005555	1.000960	0.004312	0.710230
-22.554761	-1.962084	1.005965	0.004363	0.710218
-22.458393	-1.975351	1.010970	0.004345	0.710226
-22.140165	-2.034355	1.015974	0.004286	0.710222
-22.369013	-1.994635	1.020979	0.004328	0.710220
-22.084914	-2.040804	1.025984	0.004275	0.710229
-22.358995	-2.106048	1.030989	0.004326	0.710001
-23.371197	-1.976905	1.035994	0.004515	0.709899
-23.489448	-1.955133	1.040998	0.004537	0.709900
-23.601703	-1.936967	1.046003	0.004557	0.709897
-23.223561	-2.001223	1.051008	0.004487	0.709903
-23.197529	-2.010623	1.056013	0.004482	0.709894
-23.375156	-1.976281	1.061018	0.004515	0.709899
-23.296886	-2.025898	1.066022	0.004500	0.709828
-24.171744	-1.987380	1.071027	0.004663	0.709594
-23.936690	-2.023567	1.076032	0.004619	0.709605
-24.335139	-1.956824	1.081037	0.004693	0.709597
-24.138532	-1.989906	1.086042	0.004657	0.709601
-23.886248	-2.034274	1.091046	0.004610	0.709602
-24.435789	-1.940101	1.096051	0.004712	0.709595
-24.083729	-2.027409	1.101056	0.004646	0.709546
-25.055129	-1.993316	1.106061	0.004827	0.709268
-25.088165	-1.984077	1.111066	0.004833	0.709275
-25.112785	-1.980315	1.116070	0.004838	0.709274
-24.976015	-2.008819	1.121075	0.004812	0.709265
-25.024568	-1.995372	1.126080	0.004821	0.709275
-25.202080	-1.966862	1.131085	0.004854	0.709269
-24.970794	-2.005346	1.136090	0.004811	0.709275
-25.328428	-2.083095	1.141094	0.004877	0.708992
-26.285387	-1.928787	1.146099	0.005055	0.708959
-25.803462	-2.009402	1.151104	0.004966	0.708970
-25.573778	-2.053448	1.156109	0.004923	0.708964
-26.078942	-1.961445	1.161114	0.005017	0.708968
-25.913635	-1.992929	1.166118	0.004986	0.708964
-25.844168	-2.006673	1.171123	0.004973	0.708962
-26.504688	-2.038173	1.176128	0.005096	0.708663
-26.925097	-1.971440	1.181133	0.005174	0.708647
-26.866327	-1.981056	1.186138	0.005163	0.708649
-26.495325	-2.045960	1.191142	0.005094	0.708651
-27.084073	-1.943387	1.196147	0.005203	0.708647
-26.744459	-2.000828	1.201152	0.005140	0.708653
-26.428357	-2.059766	1.206157	0.005081	0.708648
-27.374491	-2.033291	1.211162	0.005257	0.708363
-27.589350	-1.995939	1.216166	0.005297	0.708361
-27.777361	-1.965630	1.221171	0.005332	0.708355
-27.479090	-2.014031	1.226176	0.005276	0.708365
-27.999482	-1.926751	1.231181	0.005373	0.708354
-27.855586	-1.951693	1.236186	0.005346	0.708356
-27.557751	-2.002120	1.241190	0.005291	0.708361
-28.200581	-2.032509	1.246195	0.005410	0.708071
-28.642708	-1.977114	1.251200	0.005493	0.708024
-28.483722	-2.010312	1.256205	0.005463	0.708014
-28.736143	-1.962645	1.261210	0.005510	0.708020
-28.678118	-1.972597	1.266214	0.005499	0.708021
-28.420273	-2.020726	1.271219	0.005451	0.708017
-28.207858	-2.054221	1.276224	0.005411	0.708026
-29.072494	-2.036607	1.281229	0.005572	0.707752
-29.413357	-1.998350	1.286234	0.005636	0.707707
-28.856922	-2.095411	1.291238	0.005532	0.707711
-29.645476	-1.959710	1.296243	0.005679	0.707702
-29.816609	-1.925284	1.301248	0.005710	0.707710
-29.300276	-2.020918	1.306253	0.005614	0.707703
-29.360412	-2.009229	1.311258	0.005625	0.707705
-29.913649	-2.050462	1.316262	0.005728	0.707424
-30.611159	-1.950812	1.321267	0.005858	0.707375
-30.299031	-2.001655	1.326272	0.005800	0.707385
-30.312595	-2.001572	1.331277	0.005802	0.707380
-30.463609	-1.974388	1.336282	0.005830	0.707381
-30.174568	-2.025589	1.341286	0.005776	0.707382
-30.433450	-1.980698	1.346291	0.005825	0.707380
-30.384406	-2.086750	1.351296	0.005815	0.707184
-31.048514	-2.018423	1.356301	0.005939	0.707084
-31.256830	-1.981066	1.361306	0.005978	0.707085
-31.345371	-1.962256	1.366310	0.005994	0.707091
-31.202460	-1.992973	1.371315	0.005967	0.707081
-30.801872	-2.060011	1.376320	0.005893	0.707089
-31.265315	-1.982201	1.381325	0.005979	0.707080
-31.688831	-2.044670	1.386330	0.006058	0.706803
-31.674539	-2.068468	1.391334	0.006055	0.706761
-31.857054	-2.039166	1.396339	0.006089	0.706754
-32.189096	-1.974358	1.401344	0.006151	0.706766
-32.231351	-1.973316	1.406349	0.006158	0.706753
-32.129456	-1.988408	1.411354	0.006139	0.706759
-32.032743	-2.004907	1.416358	0.006121	0.706761
-32.750107	-2.021308	1.421363	0.006255	0.706471
-32.805821	-2.020427	1.426368	0.006265	0.706453
-33.079242	-1.975115	1.431373	0.006316	0.706446
-32.751015	-2.032566	1.436378	0.006255	0.706449
-32.630451	-2.052928	1.441382	0.006232	0.706451
-33.224784	-1.949724	1.446387	0.006343	0.706446
-32.947928	-1.994524	1.451392	0.006291	0.706455
-32.935082	-2.136419	1.456397	0.006289	0.706174
-33.724075	-2.015362	1.461402	0.006435	0.706135
-33.883359	-1.987130	1.466406	0.006465	0.706135
-33.503722	-2.058247	1.471411	0.006394	0.706128
-33.318157	-2.087051	1.476416	0.006360	0.706137
-33.665380	-2.029864	1.481421	0.006424	0.706128
-34.016370	-2.019545	1.486426	0.006489	0.706023
-34.461159	-2.016515	1.491430	0.006572	0.705870
-34.608243	-1.993250	1.496435	0.006599	0.705864
-34.835764	-1.948976	1.501440	0.006642	0.705872
-34.745214	-1.969267	1.506445	0.006625	0.705863
-34.478517	-2.016453	1.511450	0.006575	0.705864
-34.650171	-1.981903	1.516454	0.006607	0.705872
-34.781073	-2.007725	1.521459	0.006631	0.705774
-35.363157	-2.021805	1.526464	0.006740	0.705537
-35.435469	-2.013920	1.531469	0.006753	0.705527
-35.510178	-1.999636	1.536474	0.006767	0.705529
-35.131467	-2.065663	1.541478	0.006696	0.705532
-35.408610	-2.018556	1.546483	0.006748	0.705527
-35.690827	-1.963758	1.551488	0.006800	0.705537
-35.407475	-2.092195	1.556493	0.006747	0.705380
-36.282671	-2.017026	1.561498	0.006910	0.705217
-36.382081	-1.997216	1.566502	0.006929	0.705222
-36.555687	-1.972204	1.571507	0.006961	0.705210
-36.135353	-2.042745	1.576512	0.006883	0.705219
-36.393143	-2.000326	1.581517	0.006930	0.705212
-36.406707	-1.995700	1.586522	0.006933	0.705217
-36.262271	-2.103798	1.591526	0.006906	0.705051
-37.378772	-1.984916	1.596531	0.007114	0.704890
-37.226997	-2.007787	1.601536	0.007085	0.704898
-37.424288	-1.976806	1.606541	0.007122	0.704890
-37.420523	-1.976627	1.611546	0.007121	0.704892
-37.155463	-2.023718	1.616550	0.007072	0.704892
-37.262896	-2.007011	1.621555	0.007092	0.704888
-37.170819	-2.090127	1.626560	0.007075	0.704753
-38.083817	-2.007983	1.631565	0.007244	0.704591
-37.957739	-2.029180	1.636570	0.007221	0.704594
-37.961744	-2.025718	1.641574	0.007222	0.704599
-38.168926	-1.992275	1.646579	0.007260	0.704593
-37.926710	-2.031268	1.651584	0.007215	0.704601
-38.189186	-1.988086	1.656589	0.007264	0.704594
-38.245440	-2.089989	1.661594	0.007274	0.704369
-39.075973	-1.992887	1.666598	0.007429	0.704266
-39.167289	-1.979204	1.671603	0.007445	0.704261
-38.808875	-2.038642	1.676608	0.007379	0.704270
-39.194547	-1.973381	1.681613	0.007450	0.704263
-39.477749	-1.922282	1.686618	0.007503	0.704265
-38.931118	-2.018598	1.691622	0.007401	0.704267
-39.067674	-2.052348	1.696627	0.007427	0.704150
-39.979240	-1.984384	1.701632	0.007596	0.703960
-39.810391	-2.017501	1.706637	0.007565	0.703954
-40.021847	-1.978340	1.711642	0.007604	0.703957
-39.914609	-1.995948	1.716646	0.007584	0.703960
-40.056347	-1.973740	1.721651	0.007610	0.703954
-39.945488	-1.990021	1.726656	0.007589	0.703961
-39.741563	-2.069699	1.731661	0.007551	0.703874
-40.819454	-1.994937	1.736666	0.007752	0.703637
-40.617467	-2.028934	1.741670	0.007714	0.703641
-40.972014	-1.969717	1.746675	0.007780	0.703633
-40.895526	-1.978597	1.751680	0.007766	0.703643
-40.816357	-1.994954	1.756685	0.007751	0.703639
-40.904683	-1.979404	1.761690	0.007767	0.703639
-40.843934	-2.000481	1.766694	0.007756	0.703618
-41.739370	-1.981115	1.771699	0.007923	0.703335
-41.702141	-1.980525	1.776704	0.007916	0.703350
-41.656887	-1.990835	1.781709	0.007907	0.703345
-41.694259	-1.983170	1.786714	0.007914	0.703348
-41.556709	-2.006261	1.791718	0.007888	0.703351
-41.647580	-1.993775	1.796723	0.007905	0.703343
-41.769425	-1.966490	1.801728	0.007928	0.703355
-42.368967	-2.026547	1.806733	0.008039	0.703018
-42.603606	-1.989356	1.811738	0.008083	0.703008
-42.382340	-2.025132	1.816742	0.008042	0.703016
-42.612158	-1.988028	1.821747	0.008084	0.703008
-42.922833	-1.927509	1.826752	0.008142	0.703019
-42.529178	-2.002128	1.831757	0.008069	0.703010
-42.665912	-1.977214	1.836762	0.008094	0.703011
-42.791913	-2.074529	1.841766	0.008118	0.702769
-43.630315	-1.962527	1.846771	0.008274	0.702694
-43.407344	-1.999034	1.851776	0.008232	0.702701
-43.293207	-2.020888	1.856781	0.008211	0.702698
-43.520263	-1.981224	1.861786	0.008253	0.702696
-43.430172	-1.993926	1.866790	0.008236	0.702703
-43.680636	-1.954336	1.871795	0.008283	0.702693
-43.736050	-2.065104	1.876800	0.008293	0.702449
-44.429765	-1.977407	1.881805	0.008422	0.702377
-44.509028	-1.962661	1.886810	0.008437	0.702378
-44.272626	-2.003340	1.891814	0.008392	0.702381
-44.522044	-1.964011	1.896819	0.008439	0.702371
-44.126495	-2.030321	1.901824	0.008365	0.702380
-44.431740	-1.976755	1.906829	0.008422	0.702378
-44.768772	-2.021557	1.911834	0.008485	0.702166
-45.282760	-1.969356	1.916838	0.008580	0.702087
-45.373173	-1.956557	1.921843	0.008597	0.702080
-45.197170	-1.984348	1.926848	0.008564	0.702087
-45.504958	-1.931137	1.931853	0.008621	0.702084
-45.497730	-1.933006	1.936858	0.008620	0.702083
-45.238354	-1.977976	1.941862	0.008571	0.702086
-45.556009	-1.977974	1.946867	0.008631	0.701972
-46.105436	-1.986735	1.951872	0.008733	0.701756
-45.909543	-2.023781	1.956877	0.008696	0.701752
-46.372541	-1.940931	1.961882	0.008782	0.701752
-46.272159	-1.956014	1.966886	0.008764	0.701758
-46.308287	-1.955937	1.971891	0.008770	0.701746
-46.105929	-1.986540	1.976896	0.008732	0.701757
-45.848033	-2.083839	1.981901	0.008684	0.701653
-46.851459	-2.008716	1.986906	0.008871	0.701443
-46.911236	-1.995093	1.991910	0.008882	0.701449
-47.166201	-1.952143	1.996915	0.008929	0.701444
-46.848709	-2.008626	2.001920	0.008870	0.701445

-46.878848	-2.004607	2.011917	0.008876	0.701442
-47.720035	-1.977063	2.021914	0.009032	0.701195
-47.958280	-1.967069	2.031910	0.009076	0.701129
-48.009659	-1.959725	2.041907	0.009086	0.701126
-47.771183	-2.000857	2.051904	0.009041	0.701129
-47.700144	-2.014413	2.061901	0.009028	0.701127
-47.322988	-1.948364	2.071898	0.008957	0.701398
-47.187097	-2.001148	2.081894	0.008932	0.701340
-47.187251	-1.950999	2.091891	0.008932	0.701442
-46.716259	-2.034587	2.101888	0.008844	0.701443
-47.160969	-1.954842	2.111885	0.008927	0.701444
-47.139839	-1.959963	2.121882	0.008923	0.701442
-47.079910	-1.971384	2.131878	0.008911	0.701441
-46.937096	-1.997311	2.141875	0.008884	0.701440
-47.030471	-1.932426	2.151872	0.008902	0.701538
-46.023206	-2.006971	2.161869	0.008714	0.701751
-46.331921	-1.952283	2.171866	0.008771	0.701751
-46.056154	-2.003689	2.181862	0.008720	0.701747
-46.297623	-1.960604	2.191859	0.008765	0.701747
-45.447947	-1.989871	2.201856	0.008606	0.701995
-45.394122	-1.958488	2.211853	0.008596	0.702078
-44.988332	-2.029946	2.221850	0.008520	0.702080
-45.124559	-2.005586	2.231846	0.008546	0.702080
-45.182153	-1.933048	2.241843	0.008556	0.702207
-44.404005	-1.988507	2.251840	0.008411	0.702375
-44.577422	-1.956822	2.261837	0.008443	0.702377
-44.386603	-1.991461	2.271834	0.008407	0.702376
-43.828380	-1.963274	2.281830	0.008303	0.702635
-43.524755	-1.989104	2.291827	0.008247	0.702692
-43.360007	-2.015345	2.301824	0.008216	0.702699
-43.729330	-1.938799	2.311821	0.008284	0.702721
-42.718426	-1.976544	2.321818	0.008096	0.703009
-42.701493	-1.979681	2.331814	0.008093	0.703009
-42.832476	-1.956489	2.341811	0.008117	0.703009
-42.305309	-1.960058	2.351808	0.008019	0.703192
-41.885244	-1.958905	2.361805	0.007940	0.703346
-41.676130	-1.995875	2.371802	0.007901	0.703347
-41.813800	-1.973311	2.381798	0.007927	0.703343
-41.017808	-1.981587	2.391795	0.007778	0.703614
-40.682832	-2.030190	2.401792	0.007716	0.703636
-41.013811	-1.969219	2.411789	0.007777	0.703641
-40.900596	-1.946656	2.421786	0.007756	0.703727
-40.205571	-1.959787	2.431782	0.007626	0.703951
-39.980270	-1.998208	2.441779	0.007584	0.703955
-39.991392	-1.995802	2.451776	0.007586	0.703956
-39.465801	-1.960246	2.461773	0.007488	0.704217
-39.144206	-1.995097	2.471770	0.007428	0.704263
-39.138089	-1.995066	2.481766	0.007427	0.704265
-39.104996	-1.958374	2.491763	0.007420	0.704351
-38.248364	-1.987951	2.501760	0.007261	0.704600
-38.306921	-1.977632	2.511757	0.007271	0.704600
-38.353866	-1.972601	2.521754	0.007280	0.704594
-37.871669	-1.934459	2.531750	0.007190	0.704844
-37.401564	-1.993895	2.541747	0.007102	0.704893
-37.223114	-2.024424	2.551744	0.007069	0.704896
-37.436416	-1.929188	2.561741	0.007108	0.705012
-36.575718	-1.982181	2.571738	0.006948	0.705214
-36.527145	-1.992277	2.581734	0.006939	0.705212
-36.487862	-1.999514	2.591731	0.006931	0.705212
-35.982646	-1.951147	2.601728	0.006837	0.705491
-35.512260	-2.016041	2.611725	0.006749	0.705529
-35.473186	-2.023280	2.621722	0.006742	0.705529
-35.743769	-1.935372	2.631718	0.006792	0.705609
-34.538565	-2.022053	2.641715	0.006568	0.705867
-34.694130	-1.993358	2.651712	0.006596	0.705869
-34.854556	-1.963135	2.661709	0.006626	0.705873
-34.395855	-1.949628	2.671706	0.006541	0.706065
-34.288293	-1.937519	2.681702	0.006520	0.706128
-33.939541	-1.997541	2.691699	0.006455	0.706133
-33.842431	-1.936809	2.701696	0.006437	0.706290
-33.037366	-2.001572	2.711693	0.006287	0.706449
-33.190428	-1.974294	2.721690	0.006315	0.706449
-33.221453	-1.956053	2.731686	0.006321	0.706475
-32.533826	-1.940745	2.741683	0.006193	0.706752
-32.359350	-1.970519	2.751680	0.006160	0.706755
-32.296469	-1.980367	2.761677	0.006148	0.706758
-31.679358	-1.957217	2.771674	0.006033	0.707026
-31.506078	-1.960004	2.781670	0.006001	0.707083
-31.194453	-2.014724	2.791667	0.005943	0.707085
-31.384811	-1.943129	2.801664	0.005978	0.707161
-30.165118	-2.049087	2.811661	0.005751	0.707385
-30.660394	-1.961799	2.821658	0.005843	0.707383
-30.532999	-1.986489	2.831654	0.005819	0.707379
-29.844987	-1.997034	2.841651	0.005690	0.707604
-29.776196	-1.959207	2.851648	0.005677	0.707705
-29.523328	-2.002518	2.861645	0.005630	0.707709
-29.644587	-1.954422	2.871642	0.005653	0.707763
-28.687565	-1.999356	2.881638	0.005474	0.708015
-28.741164	-1.988364	2.891635	0.005484	0.708018
-28.756775	-1.985077	2.901632	0.005487	0.708019
-28.076210	-1.995197	2.911629	0.005360	0.708243
-27.918870	-1.967019	2.921626	0.005330	0.708356
-27.698380	-2.007988	2.931622	0.005289	0.708353
-27.877929	-1.967611	2.941619	0.005322	0.708370
-26.901671	-2.004462	2.951616	0.005141	0.708645
-26.698046	-2.039540	2.961613	0.005103	0.708647
-26.973836	-1.989928	2.971610	0.005154	0.708649
-26.884657	-1.948087	2.981606	0.005137	0.708765
-25.922422	-2.020874	2.991603	0.004958	0.708963
-25.995994	-2.007609	3.001600	0.004971	0.708963
-25.987907	-2.009247	3.011597	0.004969	0.708963
-25.462732	-1.969301	3.021594	0.004871	0.709231
-25.224595	-1.994401	3.031590	0.004827	0.709266
-25.440397	-1.954778	3.041587	0.004867	0.709269
-24.835757	-1.978138	3.051584	0.004754	0.709438
-24.293477	-1.993802	3.061581	0.004653	0.709600
-24.098312	-2.028930	3.071578	0.004617	0.709600
-24.476745	-1.962242	3.081574	0.004687	0.709598
-23.615547	-1.967816	3.091571	0.004526	0.709895
-23.629261	-1.963185	3.101568	0.004529	0.709899
-23.470102	-1.991780	3.111565	0.004499	0.709899
-23.123791	-1.953040	3.121562	0.004434	0.710100
-22.520664	-1.998737	3.131558	0.004322	0.710224
-22.738075	-1.959375	3.141555	0.004362	0.710226
-22.548629	-1.961539	3.151552	0.004327	0.710289
-21.718548	-1.984019	3.161549	0.004172	0.710540
-21.760445	-1.977572	3.171546	0.004180	0.710538
-21.813788	-1.969477	3.181542	0.004189	0.710536
-21.159268	-1.959182	3.191539	0.004067	0.710790
-20.611621	-2.013006	3.201536	0.003965	0.710877
-20.562949	-2.021522	3.211533	0.003956	0.710878
-20.765209	-1.985721	3.221530	0.003993	0.710878
-20.364706	-1.927518	3.231526	0.003919	0.711137
-20.326705	-1.930022	3.241523	0.003911	0.711146
-19.905488	-2.004012	3.251520	0.003833	0.711148
-19.487062	-1.960541	3.261517	0.003755	0.711384
-19.242946	-1.964084	3.271514	0.003709	0.711464
-18.979082	-2.011604	3.281510	0.003660	0.711463
-19.242009	-1.917326	3.291507	0.003709	0.711558
-18.190002	-2.000727	3.301504	0.003513	0.711766
-18.325527	-1.974388	3.311501	0.003538	0.711771
-18.189494	-2.001485	3.321498	0.003512	0.711765
-17.878474	-1.912700	3.331494	0.003454	0.712053
-17.364272	-1.981569	3.341491	0.003358	0.712099
-17.000723	-2.046454	3.351488	0.003290	0.712099
-17.246454	-1.959941	3.361485	0.003336	0.712184
-16.543574	-1.980570	3.371482	0.003205	0.712393
-16.399687	-2.006831	3.381478	0.003178	0.712392
-16.491689	-1.990285	3.391475	0.003195	0.712393
-15.748741	-1.998400	3.401472	0.003056	0.712641
-15.880652	-1.934799	3.411469	0.003081	0.712721
-15.526456	-1.998564	3.421466	0.003015	0.712720
-15.706412	-1.912625	3.431462	0.003048	0.712827
-14.522971	-2.019738	3.441459	0.002828	0.713034
-14.733643	-1.981542	3.451456	0.002867	0.713036
-14.695657	-1.988702	3.461453	0.002859	0.713035
-14.051862	-1.971843	3.471450	0.002739	0.713297
-13.939653	-1.955580	3.481446	0.002718	0.713370
-13.834379	-1.974923	3.491443	0.002699	0.713369
-13.718110	-1.957847	3.501440	0.002677	0.713444
-13.061187	-1.962617	3.511437	0.002554	0.713668
-12.966381	-1.980292	3.521434	0.002536	0.713667
-13.392487	-1.907572	3.531430	0.002616	0.713661
-12.237006	-1.964752	3.541427	0.002400	0.713957
-12.223019	-1.953680	3.551424	0.002397	0.713984
-12.191222	-1.960799	3.561421	0.002391	0.713981
-11.907257	-1.931132	3.571418	0.002338	0.714141
-11.161743	-1.991211	3.581414	0.002199	0.714286
-11.254949	-1.974963	3.591411	0.002217	0.714286
-11.159244	-1.991224	3.601408	0.002199	0.714287
-10.717051	-1.925258	3.611405	0.002116	0.714575
-10.324018	-1.973623	3.621402	0.002043	0.714619
-10.392856	-1.962778	3.631398	0.002055	0.714616
-10.090819	-1.963449	3.641395	0.001999	0.714722
-9.446008	-1.978597	3.651392	0.001879	0.714920
-9.340258	-1.998417	3.661389	0.001859	0.714919
-9.511541	-1.967790	3.671386	0.001891	0.714919
-8.979130	-1.931933	3.681382	0.001791	0.715179
-8.426555	-2.000658	3.691379	0.001688	0.715238
-8.518583	-1.983282	3.701376	0.001705	0.715240
-8.459005	-1.956631	3.711373	0.001694	0.715315
-7.642602	-1.980892	3.721370	0.001542	0.715555
-7.497333	-2.007514	3.731366	0.001515	0.715554
-7.415935	-2.023076	3.741363	0.001499	0.715552
-7.278874	-1.962008	3.751360	0.001474	0.715722
-6.181732	-2.071124	3.761357	0.001269	0.715893
-6.430370	-2.026643	3.771354	0.001315	0.715894
-6.579919	-2.004739	3.781350	0.001343	0.715885
-6.198544	-2.006976	3.791347	0.001272	0.716016
-5.560028	-2.057403	3.801344	0.001153	0.716141
-5.956797	-1.987644	3.811341	0.001226	0.716140
-5.718962	-2.028504	3.821338	0.001182	0.716143
-5.253306	-1.956052	3.831334	0.001095	0.716451
-4.838637	-2.026864	3.841331	0.001018	0.716458
-5.039528	-1.991915	3.851328	0.001055	0.716456
-4.298722	-2.027757	3.861325	0.000917	0.716647
-4.090543	-2.006019	3.871322	0.000878	0.716764
-4.063072	-2.010675	3.881318	0.000873	0.716764
-3.923227	-2.032500	3.891315	0.000847	0.716771
-3.298665	-1.981053	3.901312	0.000730	0.717093
-2.912034	-2.049630	3.911309	0.000658	0.717094
-3.056050	-2.024890	3.921306	0.000685	0.717092
-2.924897	-1.994333	3.931302	0.000660	0.717199
-2.295062	-2.011289	3.941299	0.000543	0.717388
-2.263317	-2.018088	3.951296	0.000536	0.717386
-2.152486	-2.035770	3.961293	0.000516	0.717390
-2.117991	-1.887628	3.971290	0.000509	0.717696
-1.684677	-1.956333	3.981286	0.000428	0.717713
-1.767682	-1.941511	3.991283	0.000443	0.717713
-1.350951	-1.863778	4.001280	0.000366	0.718014
-1.056181	-1.909348	4.011277	0.000311	0.718028
-1.124750	-1.891363	4.021274	0.000323	0.718040
-1.061626	-1.739945	4.031270	0.000311	0.718361
-1.096445	-1.735326	4.041267	0.000318	0.718359
-0.876914	-1.676955	4.051264	0.000276	0.718551
-0.712616	-1.654362	4.061261	0.000246	0.718654
-0.550052	-1.619219	4.071258	0.000215	0.718781
-0.456002	-1.540542	4.081254	0.000197	0.718970
-0.589308	-1.463618	4.091251	0.000222	0.719075
-0.597305	-1.357144	4.101248	0.000223	0.719282
-0.630836	-1.256872	4.111245	0.000229	0.719469
-0.493234	-1.208927	4.121242	0.000204	0.719612
-0.688815	-1.031744	4.131238	0.000240	0.719893
-0.347285	-1.012808	4.141235	0.000176	0.720050
-0.203514	-0.944439	4.151232	0.000149	0.720236
-0.177834	-0.795615	4.161229	0.000144	0.720538
0.007712	-0.730769	4.171226	0.000109	0.720731
-0.211731	-0.588351	4.181222	0.000150	0.720935
-0.089328	-0.509548	4.191219	0.000127	0.721133
-0.104172	-0.357171	4.201216	0.000129	0.721428
-0.027131	-0.245538	4.211213	0.000115	0.721675
-0.029394	-0.106303	4.221210	0.000115	0.721948
-0.063194	0.035814	4.231206	0.000121	0.722216
-0.009517	0.168816	4.241203	0.000111	0.722496
0.000000	0.345691	4.251200	0.000109	0.722847

0.239919	0.925322	4.256205	0.000063	0.724068
0.382019	2.159493	4.261210	0.000036	0.726532
0.643436	3.971699	4.266214	-0.000014	0.730153
0.877526	6.339386	4.271219	-0.000059	0.734820
1.430325	9.161825	4.276224	-0.000164	0.740438
1.895587	12.482781	4.281229	-0.000253	0.746932
2.610867	16.219543	4.286234	-0.000389	0.754235
3.565449	20.323294	4.291238	-0.000569	0.762231
4.404089	24.854106	4.296243	-0.000728	0.770893
5.696631	29.691147	4.301248	-0.000972	0.780161
6.994934	34.876614	4.306253	-0.001217	0.789947
10.473719	40.022858	4.311258	-0.001869	0.800228
12.246339	45.818763	4.316262	-0.002202	0.810985
13.533749	51.989856	4.321267	-0.002446	0.822101
14.818715	58.459810	4.326272	-0.002690	0.833575
15.958949	65.163654	4.331277	-0.002907	0.845242
16.878717	72.136992	4.336282	-0.003082	0.857132
18.635261	79.151907	4.341286	-0.003414	0.869166
19.814128	86.468556	4.346291	-0.003639	0.881358
20.953467	93.968758	4.351296	-0.003856	0.893662
21.955452	101.646688	4.356301	-0.004047	0.906040
23.300788	109.427512	4.361306	-0.004303	0.918501
24.683889	117.305934	4.366310	-0.004566	0.930954
25.407776	125.414018	4.371315	-0.004706	0.943413
26.960026	133.499457	4.376320	-0.005000	0.955891
27.722269	141.784878	4.381325	-0.005148	0.968298
28.707170	150.131482	4.386330	-0.005337	0.980692
29.497164	158.587919	4.391334	-0.005489	0.993039
30.370193	167.052008	4.396339	-0.005657	1.005265
31.342098	175.546152	4.401344	-0.005844	1.017410
32.882275	183.975302	4.406349	-0.006136	1.029457
33.656030	192.585072	4.411354	-0.006286	1.041428
34.241296	201.248628	4.416358	-0.006401	1.053292
34.923125	209.905034	4.421363	-0.006534	1.065036
35.730243	218.583409	4.426368	-0.006690	1.076709
36.408993	227.238075	4.431373	-0.006822	1.088197
37.104345	235.925819	4.436378	-0.006957	1.099610
37.843454	244.600621	4.441382	-0.007100	1.110899
38.764048	253.222289	4.446387	-0.007277	1.122046
39.797819	261.860704	4.451392	-0.007476	1.133128
40.961285	270.456275	4.456397	-0.007698	1.144077
42.253740	279.093369	4.461402	-0.007944	1.154999
43.021372	287.742954	4.466406	-0.008093	1.165725
43.712948	296.399955	4.471411	-0.008227	1.176345
44.745288	304.980601	4.476416	-0.008425	1.186849
45.320472	313.635260	4.481421	-0.008538	1.197255
46.023491	322.249818	4.486426	-0.008675	1.207549
46.853751	330.833896	4.491430	-0.008835	1.217746
47.405158	339.447361	4.496435	-0.008943	1.227837
47.813690	348.088268	4.501440	-0.009025	1.237850
48.541133	356.607473	4.506445	-0.009166	1.247705
49.637732	365.088419	4.511450	-0.009376	1.257509
50.561172	373.573362	4.516454	-0.009554	1.267209
51.422424	382.072496	4.521459	-0.009720	1.276839
52.291810	390.546444	4.526464	-0.009887	1.286370
53.064852	399.030338	4.531469	-0.010037	1.295824
53.960810	407.499560	4.536474	-0.010209	1.305215
54.365979	416.138988	4.541478	-0.010290	1.314634
55.281813	424.541126	4.546483	-0.010466	1.323823
55.911580	432.990449	4.551488	-0.010589	1.332947
56.204495	441.451286	4.556493	-0.010649	1.341962
57.038761	449.833003	4.561498	-0.010810	1.350928
57.763564	458.212603	4.566502	-0.010951	1.359814
58.475640	466.581296	4.571507	-0.011089	1.368628
59.139093	474.984531	4.576512	-0.011218	1.377413
59.587685	483.368382	4.581517	-0.011307	1.386085
60.159119	491.769782	4.586522	-0.011419	1.394742
60.629844	500.140187	4.591526	-0.011512	1.403297
61.308156	508.471032	4.596531	-0.011644	1.411795
61.962572	516.808262	4.601536	-0.011771	1.420244
62.317763	525.167924	4.606541	-0.011843	1.428616
63.051835	533.479000	4.611546	-0.011985	1.436953
63.728047	541.766002	4.616550	-0.012116	1.445209
64.112179	550.118826	4.621555	-0.012194	1.453434
64.775249	558.419992	4.626560	-0.012322	1.461608
65.531996	566.700766	4.631565	-0.012469	1.469731
66.079684	575.044278	4.636570	-0.012576	1.477836
66.768179	583.289381	4.641574	-0.012710	1.485825
67.343397	591.593074	4.646579	-0.012823	1.493809
67.965340	599.861075	4.651584	-0.012944	1.501724
68.340124	608.152786	4.656589	-0.013019	1.509582
68.856800	616.441915	4.661594	-0.013121	1.517418
69.469286	624.664740	4.666598	-0.013240	1.525166
70.256114	632.889916	4.671603	-0.013392	1.532903
70.923765	641.136093	4.676608	-0.013522	1.540603
71.661907	649.350882	4.681613	-0.013665	1.548246
72.011858	657.663837	4.686618	-0.013736	1.555883
72.431744	665.913948	4.691622	-0.013819	1.563436
72.772160	674.165050	4.696627	-0.013888	1.570942
73.621565	682.365198	4.701632	-0.014052	1.578440
74.448669	690.533646	4.706637	-0.014211	1.585871
75.058778	698.786142	4.711642	-0.014330	1.593310
75.571235	707.004548	4.716646	-0.014431	1.600671
75.791492	715.263254	4.721651	-0.014477	1.607992
76.310947	723.495798	4.726656	-0.014580	1.615298
76.907033	731.679246	4.731661	-0.014696	1.622540
77.668379	739.888856	4.736666	-0.014843	1.629795
78.127541	748.148785	4.741670	-0.014934	1.637019
78.593383	756.326343	4.746675	-0.015026	1.644141
78.945049	764.555542	4.751680	-0.015097	1.651261
79.240896	772.780387	4.756685	-0.015158	1.658339
79.539399	780.979736	4.761690	-0.015219	1.665366
80.084073	789.166400	4.766694	-0.015326	1.672385
80.397331	797.362145	4.771699	-0.015389	1.679351
80.905883	805.530381	4.776704	-0.015490	1.686292
81.345606	813.715532	4.781709	-0.015577	1.693208
81.785505	821.891148	4.786714	-0.015664	1.700089
82.767448	829.980955	4.791718	-0.015852	1.706941
83.296170	838.177890	4.796723	-0.015956	1.713795
84.000657	846.320672	4.801728	-0.016093	1.720600
84.230648	854.517385	4.806733	-0.016141	1.727361
84.680489	862.721217	4.811738	-0.016230	1.734130
85.090468	870.882453	4.816742	-0.016312	1.740832
85.364476	879.070448	4.821747	-0.016368	1.747513
85.948115	887.234411	4.826752	-0.016482	1.754188
86.450305	895.363962	4.831757	-0.016581	1.760800
87.289961	903.475181	4.836762	-0.016743	1.767414
87.703533	911.672949	4.841766	-0.016825	1.774019
87.823548	919.856985	4.846771	-0.016853	1.780553
88.550590	927.986942	4.851776	-0.016994	1.787094
88.836234	936.224305	4.856781	-0.017053	1.793642
89.240148	944.361432	4.861786	-0.017133	1.800102
90.070134	952.428520	4.866790	-0.017293	1.806535
90.453076	960.595762	4.871795	-0.017370	1.812970
90.620135	968.794985	4.876800	-0.017406	1.819380
90.894775	976.931461	4.881805	-0.017463	1.825732
91.719328	985.038919	4.886810	-0.017622	1.832105
92.483767	993.135776	4.891814	-0.017769	1.838441
92.936974	1001.265072	4.896819	-0.017859	1.844742
93.572625	1009.407750	4.901824	-0.017983	1.851054
93.789320	1017.587586	4.906829	-0.018029	1.857323
94.304866	1025.718625	4.911834	-0.018130	1.863569
94.758067	1033.868390	4.916838	-0.018220	1.869801
95.301668	1041.993122	4.921843	-0.018326	1.876004
95.743666	1050.115461	4.926848	-0.018414	1.882172
96.146296	1058.230240	4.931853	-0.018495	1.888310
96.600628	1066.389877	4.936858	-0.018585	1.894467
97.064360	1074.500445	4.941862	-0.018676	1.900569
97.425685	1082.630927	4.946867	-0.018749	1.906655
98.078010	1090.747984	4.951872	-0.018876	1.912743
98.353529	1098.891431	4.956877	-0.018932	1.918790
98.686041	1107.016789	4.961882	-0.019000	1.924810
99.216173	1115.133050	4.966886	-0.019104	1.930827
99.655159	1123.257195	4.971891	-0.019191	1.936820
99.980279	1131.398714	4.976896	-0.019257	1.942796
100.269946	1139.521477	4.981901	-0.019316	1.948735
100.961352	1147.658962	4.986906	-0.019450	1.954710
101.552749	1155.715154	4.991910	-0.019566	1.960598
102.079254	1163.795362	4.996915	-0.019669	1.966478
102.365394	1171.945200	5.001920	-0.019728	1.972364
102.734111	1180.048435	5.006925	-0.019802	1.978209
102.949068	1188.189638	5.011930	-0.019847	1.984047
103.336991	1196.297507	5.016934	-0.019925	1.989862
103.770892	1204.409411	5.021939	-0.020011	1.995668
104.357547	1212.480525	5.026944	-0.020126	2.001444
104.661440	1220.586505	5.031949	-0.020187	2.007198
105.128182	1228.709064	5.036954	-0.020280	2.012964
105.665071	1236.805107	5.041958	-0.020385	2.018703
105.860316	1244.926958	5.046963	-0.020427	2.024407
106.342005	1253.032447	5.051968	-0.020522	2.030114
106.678373	1261.167682	5.056973	-0.020590	2.035811
106.888674	1269.276922	5.061978	-0.020634	2.041460
107.291600	1277.365010	5.066982	-0.020715	2.047099
107.793309	1285.437508	5.071987	-0.020814	2.052721
108.037215	1293.567277	5.076992	-0.020864	2.058342
108.569571	1301.620689	5.081997	-0.020969	2.063923
108.986822	1309.715855	5.087002	-0.021052	2.069507
109.820117	1317.788260	5.092006	-0.021212	2.075101
110.219516	1325.856877	5.097011	-0.021292	2.080634
110.748886	1333.958598	5.102016	-0.021396	2.086188
111.501268	1342.025096	5.107021	-0.021541	2.091725
112.002373	1350.131661	5.112026	-0.021640	2.097249
112.388141	1358.245588	5.117030	-0.021717	2.102753
112.625183	1366.377432	5.122035	-0.021767	2.108239
113.084770	1374.551301	5.127040	-0.021858	2.113762
113.236085	1382.641859	5.132045	-0.021891	2.119184
113.715630	1390.693904	5.137050	-0.021986	2.124598
114.284378	1398.746547	5.142054	-0.022097	2.130007
114.497444	1406.862608	5.147059	-0.022142	2.135411
115.002133	1414.935223	5.152064	-0.022242	2.140799
115.505213	1422.995887	5.157069	-0.022341	2.146166
115.739184	1431.127646	5.162074	-0.022390	2.151541
115.970640	1439.247921	5.167078	-0.022438	2.156895
116.485106	1447.289102	5.172083	-0.022539	2.162210
116.874756	1455.377062	5.177088	-0.022617	2.167531
116.931802	1463.514669	5.182093	-0.022633	2.172840
117.176754	1471.604019	5.187098	-0.022684	2.178123
117.793518	1479.647081	5.192102	-0.022804	2.183396
118.169738	1487.736089	5.197107	-0.022880	2.188665
118.285046	1495.911976	5.202112	-0.022906	2.193952
118.749446	1503.941983	5.207117	-0.022998	2.199165
119.227665	1511.976071	5.212122	-0.023093	2.204370
119.732563	1520.037709	5.217126	-0.023192	2.209582
120.181698	1528.117791	5.222131	-0.023281	2.214788
120.690183	1536.176078	5.227136	-0.023381	2.219974
121.121687	1544.222123	5.232141	-0.023467	2.225132
121.562230	1552.313226	5.237146	-0.023554	2.230308
122.181269	1560.398546	5.242150	-0.023675	2.235484
122.358535	1568.492421	5.247155	-0.023713	2.240615
122.958256	1576.550657	5.252160	-0.023830	2.245748
123.253383	1584.649731	5.257165	-0.023890	2.250868
123.443092	1592.762679	5.262170	-0.023931	2.255977
123.746807	1600.848418	5.267174	-0.023993	2.261066
123.763458	1608.951304	5.272179	-0.024001	2.266130
124.337480	1617.046717	5.277184	-0.024114	2.271226
124.587848	1625.156645	5.282189	-0.024166	2.276291
124.937431	1633.191332	5.287194	-0.024236	2.281308
125.390504	1641.239312	5.292198	-0.024326	2.286330
125.552688	1649.311895	5.297203	-0.024361	2.291331
125.914935	1657.396087	5.302208	-0.024434	2.296346
126.657863	1665.373666	5.307213	-0.024578	2.301316
127.020609	1673.446483	5.312218	-0.024651	2.306301
127.383017	1681.544477	5.317222	-0.024723	2.311292
127.487324	1689.648650	5.322227	-0.024748	2.316253
128.181131	1697.670777	5.327232	-0.024883	2.321203
128.222646	1705.750953	5.332237	-0.024896	2.326124
128.362153	1713.861992	5.337242	-0.024927	2.331061
128.989452	1721.915161	5.342246	-0.025049	2.335992
129.163693	1729.990024	5.347251	-0.025087	2.340889
129.677631	1738.039882	5.352256	-0.025188	2.345789
130.210733	1746.093443	5.357261	-0.025293	2.350681
130.798942	1754.180914	5.362266	-0.025407	2.355589
131.209430	1762.243393	5.367270	-0.025489	2.360456
131.369437	1770.294583	5.372275	-0.025524	2.365287
131.891224	1778.366128	5.377280	-0.025627	2.370149
132.185657	1786.446272	5.382285	-0.025687	2.374988
132.257709	1794.544488	5.387290	-0.025706	2.379810
132.650994	1802.581773	5.392294	-0.025784	2.384611
132.932849	1810.655676	5.397299	-0.025842	2.389416
133.208215	1818.768040	5.402304	-0.025899	2.394233
133.591508	1826.778483	5.407309	-0.025975	2.398989
134.161406	1834.802061	5.412314	-0.026087	2.403757
134.469999	1842.893637	5.417318	-0.026150	2.408536
134.523004	1850.995646	5.422323	-0.026165	2.413291
134.993802	1859.050422	5.427328	-0.026258	2.418042
135.420963	1867.087529	5.432333	-0.026343	2.422769
135.973451	1875.126244	5.437338	-0.026451	2.427498
136.381862	1883.243482	5.442342	-0.026532	2.432252
136.626077	1891.333882	5.447347	-0.026583	2.436968
136.955576	1899.380672	5.452352	-0.026650	2.441657
137.190809	1907.413638	5.457357	-0.026699	2.446321
137.579583	1915.478814	5.462362	-0.026777	2.451007
137.824215	1923.562249	5.467366	-0.026828	2.455683
138.152503	1931.595740	5.472371	-0.026894	2.460328
138.645792	1939.624500	5.477376	-0.026991	2.464974
139.093543	1947.680656	5.482381	-0.027080	2.469623
139.371184	1955.768099	5.487386	-0.027137	2.474269
139.759666	1963.811938	5.492390	-0.027215	2.478889
140.154281	1971.851323	5.497395	-0.027294	2.483498
140.447582	1979.940710	5.502400	-0.027353	2.488120
140.799487	1987.993175	5.507405	-0.027424	2.492716
141.179996	1996.050431	5.512410	-0.027501	2.497309
141.469059	2004.119619	5.517414	-0.027560	2.501893
141.654261	2012.168980	5.522419	-0.027599	2.506450
142.035293	2020.271774	5.527424	-0.027676	2.511043
142.524098	2028.320288	5.532429	-0.027772	2.515605
142.613728	2036.384960	5.537434	-0.027794	2.520138
142.963445	2044.400060	5.542438	-0.027865	2.524655
143.292142	2052.447503	5.547443	-0.027931	2.529180
143.682393	2060.539794	5.552448	-0.028009	2.533726
143.897538	2068.601009	5.557453	-0.028055	2.538234
144.394975	2076.616162	5.562458	-0.028152	2.542728
144.728096	2084.679575	5.567462	-0.028220	2.547230
144.767786	2092.764718	5.572467	-0.028233	2.551715
145.262232	2100.807242	5.577472	-0.028330	2.556201
145.557217	2108.845810	5.582477	-0.028390	2.560662
145.753258	2116.893480	5.587482	-0.028432	2.565114
146.225097	2124.939035	5.592486	-0.028525	2.569575
146.589849	2132.992414	5.597491	-0.028598	2.574026
146.692515	2141.082558	5.602496	-0.028623	2.578471
146.838582	2149.141937	5.607501	-0.028655	2.582895
147.333870	2157.168172	5.612506	-0.028753	2.587317
147.857995	2165.275275	5.617510	-0.028856	2.591777
147.842174	2173.467931	5.622515	-0.028858	2.596240
148.267907	2181.449152	5.627520	-0.028943	2.600609
148.687867	2189.421471	5.632525	-0.029026	2.604967
149.191382	2197.421543	5.637530	-0.029126	2.609337
149.538389	2205.492238	5.642534	-0.029195	2.613727
149.933583	2213.504544	5.647539	-0.029274	2.618082
150.517942	2221.524484	5.652544	-0.029388	2.622447
150.863214	2229.578303	5.657549	-0.029458	2.626806
151.108140	2237.648755	5.662554	-0.029509	2.631160
151.673414	2245.717279	5.667558	-0.029620	2.635527
151.726106	2253.758832	5.672563	-0.029635	2.639839
152.104361	2261.786880	5.677568	-0.029711	2.644157
152.385257	2269.831404	5.682573	-0.029768	2.648471
152.472128	2277.939552	5.687578	-0.029790	2.652800
152.669018	2285.999174	5.692582	-0.029832	2.657102
153.073779	2293.999083	5.697587	-0.029912	2.661379
153.329613	2302.063168	5.702592	-0.029965	2.665674
153.414141	2310.133451	5.707597	-0.029986	2.669954
153.819890	2318.225148	5.712602	-0.030067	2.674259
153.996742	2326.257764	5.717606	-0.030106	2.678511
154.325355	2334.247019	5.722611	-0.030172	2.682743
154.454512	2342.324755	5.727616	-0.030201	2.687002
154.912917	2350.346086	5.732621	-0.030292	2.691246
155.258390	2358.417135	5.737626	-0.030362	2.695502
155.210804	2366.471287	5.742630	-0.030358	2.699718
155.666196	2374.481436	5.747635	-0.030448	2.703935
155.790560	2382.555261	5.752640	-0.030477	2.708159
156.028642	2390.616228	5.757645	-0.030527	2.712376
156.193059	2398.672243	5.762650	-0.030562	2.716579
156.538448	2406.696491	5.767654	-0.030632	2.720771
156.637894	2414.733593	5.772659	-0.030656	2.724948
156.952099	2422.778766	5.777664	-0.030720	2.729135
157.309589	2430.837408	5.782669	-0.030792	2.733326
157.455916	2438.882139	5.787674	-0.030824	2.737490
157.615981	2446.946679	5.792678	-0.030859	2.741659
158.017656	2454.948453	5.797683	-0.030939	2.745803
158.542379	2462.985780	5.802688	-0.031042	2.749968
158.695908	2471.117461	5.807693	-0.031076	2.754151
158.964462	2479.143911	5.812698	-0.031132	2.758282
159.443808	2487.155481	5.817702	-0.031226	2.762411
159.532305	2495.188230	5.822707	-0.031248	2.766521
159.740465	2503.239254	5.827712	-0.031292	2.770642
159.885498	2511.290721	5.832717	-0.031325	2.774753
160.320050	2519.304651	5.837722	-0.031411	2.778856
160.399994	2527.352085	5.842726	-0.031431	2.782949
160.493620	2535.412916	5.847731	-0.031454	2.787044
160.938358	2543.469176	5.852736	-0.031542	2.791150
161.088399	2551.530761	5.857741	-0.031575	2.795236
161.315267	2559.536004	5.862746	-0.031623	2.799292
161.665340	2567.550611	5.867750	-0.031693	2.803354
161.754263	2575.596449	5.872755	-0.031715	2.807411
161.962732	2583.686274	5.877760	-0.031759	2.811491
162.308976	2591.724318	5.882765	-0.031829	2.815547
162.723494	2599.717136	5.887770	-0.031912	2.819578
162.902202	2607.780939	5.892774	-0.031950	2.823625
163.023362	2615.826716	5.897779	-0.031978	2.827655
163.481683	2623.872062	5.902784	-0.032069	2.831697
163.602428	2631.954255	5.907789	-0.032096	2.835733
164.008879	2639.920323	5.912794	-0.032177	2.839721
164.504188	2647.944356	5.917798	-0.032275	2.843738
164.529754	2656.004009	5.922803	-0.032285	2.847740
164.626712	2664.082116	5.927808	-0.032308	2.851749
164.916152	2672.140567	5.932813	-0.032368	2.855754
165.297244	2680.132591	5.937818	-0.032444	2.859726
165.555894	2688.189522	5.942822	-0.032497	2.863717
165.736433	2696.212695	5.947827	-0.032536	2.867681
166.133163	2704.287707	5.952832	-0.032616	2.871678
166.459890	2712.333047	5.957837	-0.032682	2.875650
166.513515	2720.358949	5.962842	-0.032697	2.879593
167.147519	2728.364004	5.967846	-0.032820	2.883551
167.300147	2736.401172	5.972851	-0.032854	2.887494
167.510571	2744.486487	5.977856	-0.032899	2.891457
167.795858	2752.545318	5.982861	-0.032957	2.895407
168.239762	2760.555547	5.987866	-0.033045	2.899335
168.660872	2768.577471	5.992870	-0.033129	2.903263
168.772014	2776.637447	5.997875	-0.033155	2.907188
169.191335	2784.695210	6.002880	-0.033238	2.911122
169.314530	2792.810670	6.007885	-0.033267	2.915063
169.604753	2800.784101	6.012890	-0.033326	2.918939
169.918173	2808.787733	6.017894	-0.033390	2.922826
170.187825	2816.822481	6.022899	-0.033445	2.926720
170.412794	2824.857388	6.027904	-0.033492	2.930606
170.424357	2832.939840	6.032909	-0.033500	2.934500
170.870892	2840.924277	6.037914	-0.033588	2.938363
171.101809	2848.977875	6.042918	-0.033637	2.942243
170.954233	2857.025722	6.047923	-0.033614	2.946096
171.353648	2865.044745	6.052928	-0.033694	2.949958
171.776544	2873.113768	6.057933	-0.033778	2.953841
171.928188	2881.129219	6.062938	-0.033812	2.957678
172.068439	2889.173409	6.067942	-0.033843	2.961524
172.470489	2897.154288	6.072947	-0.033923	2.965348
172.824012	2905.219785	6.077952	-0.033994	2.969204
173.061550	2913.275444	6.082957	-0.034044	2.973045
173.322165	2921.324725	6.087962	-0.034098	2.976879
173.634386	2929.352700	6.092966	-0.034161	2.980701
173.896187	2937.347661	6.097971	-0.034215	2.984500
174.437242	2945.396791	6.102976	-0.034321	2.988333
174.795411	2953.448710	6.107981	-0.034393	2.992153
175.333440	2961.501464	6.112986	-0.034499	2.995978
175.600117	2969.510400	6.117990	-0.034554	2.999764
176.000504	2977.513591	6.122995	-0.034634	3.003549
176.191329	2985.573623	6.128000	-0.034675	3.007345
176.359438	2993.619026	6.133005	-0.034711	3.011128
176.703249	3001.659661	6.138010	-0.034781	3.014914
177.034121	3009.707263	6.143014	-0.034848	3.018697
177.111014	3017.732041	6.148019	-0.034867	3.022452
177.346503	3025.789216	6.153024	-0.034916	3.026225
177.679838	3033.802909	6.158029	-0.034984	3.029978
178.030841	3041.851056	6.163034	-0.035054	3.033743
178.263808	3049.902751	6.168038	-0.035103	3.037499
178.503570	3057.891892	6.173043	-0.035153	3.041222
178.676283	3065.928136	6.178048	-0.035191	3.044959
178.808361	3074.002106	6.183053	-0.035220	3.048707
179.152253	3082.034729	6.188058	-0.035290	3.052442
179.393460	3090.101372	6.193062	-0.035340	3.056182
179.535264	3098.094787	6.198067	-0.035372	3.059879
180.017077	3106.116217	6.203072	-0.035467	3.063601
180.453088	3114.150950	6.208077	-0.035553	3.067322
180.439968	3122.204494	6.213082	-0.035556	3.071027
180.704708	3130.347777	6.218086	-0.035611	3.074780
180.761665	3138.327433	6.223091	-0.035627	3.078445
180.990063	3146.340944	6.228096	-0.035675	3.082129
181.347012	3154.336918	6.233101	-0.035746	3.085806
181.620217	3162.363317	6.238106	-0.035803	3.089489
181.947788	3170.399469	6.243110	-0.035869	3.093174
182.066197	3178.456691	6.248115	-0.035896	3.096855
182.270169	3186.476641	6.253120	-0.035939	3.100518
182.634503	3194.484737	6.258125	-0.036013	3.104179
182.691596	3202.515127	6.263130	-0.036029	3.107832
183.078135	3210.575326	6.268134	-0.036106	3.111508
183.264803	3218.598904	6.273139	-0.036146	3.115155
183.637379	3226.639840	6.278144	-0.036221	3.118814
183.639933	3234.661278	6.283149	-0.036226	3.122443
184.084282	3242.660363	6.288154	-0.036314	3.126077
184.355192	3250.721310	6.293158	-0.036370	3.129727
184.399141	3258.768308	6.298163	-0.036384	3.133357
184.773909	3266.819386	6.303168	-0.036459	3.136999
185.056130	3274.833482	6.308173	-0.036517	3.140616
185.235692	3282.847491	6.313178	-0.036555	3.144224
185.458748	3290.909043	6.318182	-0.036602	3.147851
185.578346	3298.937075	6.323187	-0.036630	3.151454
186.072557	3307.020452	6.328192	-0.036727	3.155095
186.246282	3315.014435	6.333197	-0.036765	3.158677
186.246629	3323.037792	6.338202	-0.036770	3.162261
186.655335	3331.040788	6.343206	-0.036852	3.165849
186.837439	3339.073422	6.348211	-0.036891	3.169436
187.240037	3347.099752	6.353216	-0.036971	3.173026
187.390434	3355.164404	6.358221	-0.037005	3.176618
187.630728	3363.166392	6.363226	-0.037055	3.180182
187.959729	3371.205655	6.368230	-0.037121	3.183763
188.059877	3379.240633	6.373235	-0.037145	3.187327
188.475221	3387.266781	6.378240	-0.037228	3.190897
188.793513	3395.326858	6.383245	-0.037292	3.194474
188.858414	3403.342249	6.388250	-0.037310	3.198017
189.172388	3411.389839	6.393254	-0.037374	3.201580
189.616335	3419.342891	6.398259	-0.037461	3.205103
190.089169	3427.392342	6.403264	-0.037555	3.208665
190.594516	3435.445098	6.408269	-0.037654	3.212227
190.978642	3443.487076	6.413274	-0.037731	3.215774
191.113227	3451.537184	6.418278	-0.037762	3.219311
191.124163	3459.547840	6.423283	-0.037769	3.222822
191.363955	3467.614511	6.428288	-0.037819	3.226362
191.623287	3475.611200	6.433293	-0.037872	3.229869
191.853755	3483.703064	6.438298	-0.037921	3.233413
192.296815	3491.759974	6.443302	-0.038009	3.236946
192.512797	3499.709190	6.448307	-0.038054	3.240419
192.692368	3507.728513	6.453312	-0.038093	3.243917
193.058336	3515.752435	6.458317	-0.038166	3.247421
193.164279	3523.767281	6.463322	-0.038191	3.250906
193.421685	3531.838878	6.468326	-0.038245	3.254419
193.712312	3539.846399	6.473331	-0.038304	3.257901
193.910520	3547.915043	6.478336	-0.038346	3.261403
193.998584	3555.914337	6.483341	-0.038368	3.264866
194.259268	3563.928971	6.488346	-0.038422	3.268339
194.529747	3572.004216	6.493350	-0.038477	3.271834
194.726179	3580.011584	6.498355	-0.038519	3.275294
194.898951	3588.038352	6.503360	-0.038557	3.278758
195.253890	3596.043568	6.508365	-0.038628	3.282215
195.373491	3604.059565	6.513370	-0.038656	3.285665
195.565600	3612.115413	6.518374	-0.038697	3.289131
195.891710	3620.146071	6.523379	-0.038763	3.292587
196.240144	3628.205953	6.528384	-0.038833	3.296053
196.348799	3636.216930	6.533389	-0.038859	3.299485
196.334267	3644.250863	6.538394	-0.038861	3.302919
196.620848	3652.287781	6.543398	-0.038920	3.306362
196.873480	3660.260063	6.548403	-0.038972	3.309773
197.152078	3668.358624	6.553408	-0.039029	3.313234
197.387105	3676.416789	6.558413	-0.039079	3.316674
197.570843	3684.364529	6.563418	-0.039118	3.320060
197.659394	3692.411877	6.568422	-0.039140	3.323482
197.840645	3700.426371	6.573427	-0.039179	3.326890
198.113505	3708.446372	6.578432	-0.039235	3.330301
198.492119	3716.502438	6.583437	-0.039311	3.333726
198.506104	3724.540206	6.588442	-0.039319	3.337127
198.745795	3732.549704	6.593446	-0.039369	3.340521
199.021372	3740.571776	6.598451	-0.039425	3.343918
199.135844	3748.608586	6.603456	-0.039452	3.347312
199.344425	3756.632942	6.608461	-0.039496	3.350701
199.667650	3764.686890	6.613466	-0.039562	3.354103
199.916748	3772.729503	6.618470	-0.039613	3.357493
200.001938	3780.726665	6.623475	-0.039635	3.360856
200.432916	3788.702505	6.628480	-0.039720	3.364218
200.500499	3796.759810	6.633485	-0.039738	3.367598
200.499973	3804.822805	6.638490	-0.039743	3.370975
200.900304	3812.864552	6.643494	-0.039823	3.374354
201.210022	3820.851934	6.648499	-0.039886	3.377703
201.491592	3828.894649	6.653504	-0.039944	3.381071
201.498364	3836.927360	6.658509	-0.039950	3.384422
201.845715	3844.929832	6.663514	-0.040020	3.387769
202.140361	3852.975548	6.668518	-0.040081	3.391128
202.355987	3861.093798	6.673523	-0.040126	3.394512
202.594080	3869.099604	6.678528	-0.040176	3.397846
202.824660	3877.073377	6.683533	-0.040224	3.401164
203.080793	3885.044653	6.688538	-0.040277	3.404478
203.374660	3893.084811	6.693542	-0.040337	3.407818
203.693803	3901.099979	6.698547	-0.040402	3.411146
203.719847	3909.169080	6.703552	-0.040412	3.414483
203.908202	3917.197270	6.708557	-0.040452	3.417805
204.185916	3925.192765	6.713562	-0.040509	3.421113
204.521298	3933.231604	6.718566	-0.040577	3.424438
204.629818	3941.243754	6.723571	-0.040602	3.427741
205.139166	3949.283600	6.728576	-0.040703	3.431066
205.467673	3957.329390	6.733581	-0.040769	3.434384
205.579392	3965.351916	6.738586	-0.040795	3.437681
205.898942	3973.367012	6.743590	-0.040860	3.440980
206.102103	3981.360423	6.748595	-0.040903	3.444262
206.308537	3989.429199	6.753600	-0.040947	3.447573
206.489745	3997.455921	6.758605	-0.040986	3.450862
206.482984	4005.511479	6.763610	-0.040990	3.454153
206.948952	4013.516509	6.768614	-0.041082	3.457436
206.936082	4021.532093	6.773619	-0.041085	3.460705
207.331364	4029.552887	6.778624	-0.041164	3.463986
207.495029	4037.618158	6.783629	-0.041200	3.467274
207.666602	4045.616815	6.788634	-0.041237	3.470533
208.132678	4053.688378	6.793638	-0.041329	3.473827
208.287098	4061.685260	6.798643	-0.041363	3.477078
208.958566	4069.663973	6.803648	-0.041494	3.480335
209.156532	4077.712025	6.808653	-0.041536	3.483602
209.459556	4085.725616	6.813658	-0.041597	3.486855
209.716726	4093.767385	6.818662	-0.041651	3.490115
209.896182	4101.781830	6.823667	-0.041689	3.493358
209.991951	4109.859019	6.828672	-0.041713	3.496621
210.391715	4117.834452	6.833677	-0.041792	3.499850
210.552569	4125.800876	6.838682	-0.041827	3.503064
210.895021	4133.881865	6.843686	-0.041897	3.506327
211.107119	4141.877965	6.848691	-0.041941	3.509549
211.400766	4149.932067	6.853696	-0.042001	3.512794
211.641928	4157.985292	6.858701	-0.042052	3.516034
211.638126	4165.981266	6.863706	-0.042056	3.519240
211.892746	4173.999327	6.868710	-0.042109	3.522460
212.161026	4182.014457	6.873715	-0.042164	3.525676
212.366413	4190.060507	6.878720	-0.042208	3.528900
212.477392	4198.092165	6.883725	-0.042234	3.532112
212.796527	4206.117202	6.888730	-0.042298	3.535325
213.001525	4214.162117	6.893734	-0.042342	3.538540
213.290478	4222.198802	6.898739	-0.042401	3.541750
213.473956	4230.198168	6.903744	-0.042441	3.544940
213.555864	4238.279881	6.908749	-0.042461	3.548157
214.037285	4246.282128	6.913754	-0.042556	3.551350
214.299451	4254.404709	6.918758	-0.042610	3.554583
214.449175	4262.384770	6.923763	-0.042643	3.557752
214.610331	4270.369611	6.928768	-0.042679	3.560921
214.919549	4278.350053	6.933773	-0.042742	3.564090
215.042964	4286.361530	6.938778	-0.042770	3.567262
215.286718	4294.422842	6.943782	-0.042821	3.570455
215.257611	4302.462981	6.948787	-0.042820	3.573629
215.567240	4310.505609	6.953792	-0.042883	3.576810
215.654269	4318.463796	6.958797	-0.042905	3.579950
215.824889	4326.499157	6.963802	-0.042942	3.583119
216.196233	4334.521791	6.968806	-0.043016	3.586286
216.429279	4342.505947	6.973811	-0.043065	3.589431
216.806107	4350.578439	6.978816	-0.043141	3.592612
217.141447	4358.618228	6.983821	-0.043208	3.595776
217.143758	4366.589251	6.988826	-0.043214	3.598901
217.450259	4374.642217	6.993830	-0.043277	3.602064
217.591321	4382.611901	6.998835	-0.043308	3.605187
217.990631	4390.631143	7.003840	-0.043388	3.608334
217.895262	4398.695404	7.008845	-0.043375	3.611482
218.042616	4406.731316	7.013850	-0.043408	3.614622
218.469216	4414.760457	7.018854	-0.043493	3.617765
218.748794	4422.743664	7.023859	-0.043550	3.620883
218.801794	4430.783265	7.028864	-0.043565	3.624015
219.061284	4438.817204	7.033869	-0.043619	3.627147
219.200292	4446.842394	7.038874	-0.043650	3.630269
219.708214	4454.930487	7.043878	-0.043750	3.633424
219.786666	4462.951382	7.048883	-0.043770	3.636537
220.066472	4470.921944	7.053888	-0.043827	3.639634
220.301824	4478.950839	7.058893	-0.043877	3.642750
220.442376	4486.939076	7.063898	-0.043908	3.645845
220.757285	4494.985386	7.068902	-0.043972	3.648964
221.157502	4503.007104	7.073907	-0.044052	3.652073
221.083766	4511.066102	7.078912	-0.044043	3.655182
221.481674	4519.088969	7.083917	-0.044123	3.658286
221.680462	4527.107832	7.088922	-0.044165	3.661381
221.916396	4535.157874	7.093926	-0.044214	3.664486
222.077643	4543.154049	7.098931	-0.044250	3.667566
222.236526	4551.166934	7.103936	-0.044285	3.670650
222.491433	4559.215266	7.108941	-0.044337	3.673747
222.411883	4567.243701	7.113946	-0.044328	3.676825
222.945068	4575.224740	7.118950	-0.044432	3.679898
223.360263	4583.211452	7.123955	-0.044515	3.682968
223.373875	4591.269597	7.128960	-0.044523	3.686052
223.670230	4599.302215	7.133965	-0.044583	3.689131
224.063688	4607.316580	7.138970	-0.044662	3.692202
224.373877	4615.356281	7.143974	-0.044725	3.695279
224.468335	4623.355328	7.148979	-0.044748	3.698333
224.578176	4631.397744	7.153984	-0.044774	3.701400
224.997673	4639.382746	7.158989	-0.044857	3.704451
225.073505	4647.411264	7.163994	-0.044877	3.707507
225.393686	4655.455528	7.168998	-0.044941	3.710573
225.525672	4663.533350	7.174003	-0.044971	3.713645
225.653564	4671.613248	7.179008	-0.045001	3.716714
225.839862	4679.547947	7.184013	-0.045041	3.719728
226.267633	4687.534150	7.189018	-0.045125	3.722764
226.575949	4695.547762	7.194022	-0.045188	3.725805
226.552909	4703.591265	7.199027	-0.045189	3.728847
226.744686	4711.607283	7.204032	-0.045230	3.731881
227.042465	4719.637390	7.209037	-0.045291	3.734921
227.225158	4727.658958	7.214042	-0.045330	3.737952
227.650320	4735.679611	7.219046	-0.045415	3.740986
227.713817	4743.669538	7.224051	-0.045432	3.743997
227.860070	4751.720597	7.229056	-0.045464	3.747031
228.165910	4759.760189	7.234061	-0.045527	3.750062
228.223760	4767.791627	7.239066	-0.045543	3.753082
228.503109	4775.862686	7.244070	-0.045600	3.756119
228.541042	4783.828500	7.249075	-0.045613	3.759109
228.826026	4791.861577	7.254080	-0.045671	3.762127
229.052191	4799.873094	7.259085	-0.045718	3.765133
229.036169	4807.909818	7.264090	-0.045721	3.768140
229.286146	4815.929546	7.269094	-0.045773	3.771145
229.420154	4823.953505	7.274099	-0.045803	3.774147
229.704352	4831.979180	7.279104	-0.045861	3.777150
229.850413	4839.965139	7.284109	-0.045893	3.780133
230.027474	4847.994186	7.289114	-0.045932	3.783130
230.457416	4856.011463	7.294118	-0.046017	3.786126
230.686286	4864.043713	7.299123	-0.046065	3.789120
230.966681	4872.092853	7.304128	-0.046123	3.792120
231.035683	4880.149035	7.309133	-0.046141	3.795115
231.155280	4888.128777	7.314138	-0.046168	3.798081
231.600795	4896.112808	7.319142	-0.046257	3.801053
231.881451	4904.079933	7.324147	-0.046314	3.804012
232.034876	4912.155128	7.329152	-0.046348	3.807007
232.280184	4920.169057	7.334157	-0.046399	3.809978
232.476730	4928.214939	7.339162	-0.046441	3.812958
232.883145	4936.224858	7.344166	-0.046522	3.815927
232.792439	4944.274428	7.349171	-0.046510	3.818898
232.986329	4952.255768	7.354176	-0.046552	3.821847
233.406668	4960.261970	7.359181	-0.046635	3.824807
233.407189	4968.287922	7.364186	-0.046641	3.827764
233.670129	4976.324097	7.369190	-0.046695	3.830728
233.923021	4984.349347	7.374195	-0.046747	3.833685
234.212548	4992.394174	7.379200	-0.046807	3.836648
234.385476	5000.391419	7.384205	-0.046844	3.839588
234.513521	5008.412667	7.389210	-0.046873	3.842535
234.948290	5016.413085	7.394214	-0.046960	3.845477
235.178736	5024.421622	7.399219	-0.047008	3.848416
235.311982	5032.491159	7.404224	-0.047038	3.851373
235.484074	5040.532415	7.409229	-0.047075	3.854319
235.496919	5048.562885	7.414234	-0.047083	3.857255
235.840760	5056.576522	7.419238	-0.047152	3.860189
236.306116	5064.580478	7.424243	-0.047244	3.863119
236.329241	5072.585259	7.429248	-0.047254	3.866039
236.370263	5080.649145	7.434253	-0.047267	3.868979
236.680897	5088.681719	7.439258	-0.047330	3.871910
237.236291	5096.934165	7.444262	-0.047439	3.874924
237.139583	5104.857440	7.449267	-0.047426	3.877803
237.225396	5112.781284	7.454272	-0.047447	3.880684
237.752944	5120.763654	7.459277	-0.047551	3.883592
238.045310	5128.783438	7.464282	-0.047611	3.886507
238.305685	5136.773990	7.469286	-0.047664	3.889408
238.297262	5144.780220	7.474291	-0.047668	3.892308
238.908311	5152.813142	7.479296	-0.047787	3.895228
239.168421	5160.864329	7.484301	-0.047841	3.898144
239.395602	5168.832615	7.489306	-0.047888	3.901029
239.588150	5176.883037	7.494310	-0.047930	3.903940
239.708323	5184.907748	7.499315	-0.047957	3.906838
239.945920	5192.931677	7.504320	-0.048007	3.909735
240.329450	5200.960390	7.509325	-0.048084	3.912636
240.368433	5208.985620	7.514330	-0.048096	3.915526
240.568217	5217.004432	7.519334	-0.048139	3.918415
240.514314	5224.995837	7.524339	-0.048134	3.921287
240.870656	5232.925813	7.529344	-0.048206	3.924142
240.874963	5241.045260	7.534349	-0.048212	3.927057
240.961059	5249.000446	7.539354	-0.048233	3.929913
241.583355	5257.068504	7.544358	-0.048354	3.932816
241.748278	5265.084892	7.549363	-0.048390	3.935690
241.825213	5273.097531	7.554368	-0.048410	3.938560
242.308940	5281.099868	7.559373	-0.048505	3.941430
242.372157	5289.102299	7.564378	-0.048522	3.944292
242.565319	5297.209274	7.569382	-0.048564	3.947190
242.960118	5305.147272	7.574387	-0.048642	3.950030
243.215949	5313.215995	7.579392	-0.048695	3.952912
243.412569	5321.285642	7.584397	-0.048737	3.955791
243.541612	5329.216233	7.589402	-0.048767	3.958618
243.889185	5337.241458	7.594406	-0.048837	3.961479
243.779394	5345.257158	7.599411	-0.048822	3.964328
243.721035	5353.316617	7.604416	-0.048816	3.967191
244.064749	5361.299014	7.609421	-0.048885	3.970031
244.466465	5369.311886	7.614426	-0.048965	3.972881
244.476064	5377.423604	7.619430	-0.048973	3.975757
244.535563	5385.403176	7.624435	-0.048989	3.978585
244.844860	5393.383237	7.629440	-0.049052	3.981415
245.146047	5401.397731	7.634445	-0.049113	3.984256
245.304012	5409.433391	7.639450	-0.049148	3.987099
245.533872	5417.467205	7.644454	-0.049196	3.989941
245.872231	5425.497564	7.649459	-0.049264	3.992782
245.819879	5433.539725	7.654464	-0.049260	3.995618
246.026309	5441.561025	7.659469	-0.049304	3.998449
245.923671	5449.546816	7.664474	-0.049290	4.001261
246.353465	5457.583931	7.669478	-0.049375	4.004097
246.671006	5465.611439	7.674483	-0.049440	4.006926
246.763552	5473.647476	7.679488	-0.049462	4.009752
246.724735	5481.685160	7.684493	-0.049460	4.012575
246.920018	5489.680111	7.689498	-0.049502	4.015384
247.214307	5497.704086	7.694502	-0.049562	4.018204
247.451266	5505.700650	7.699507	-0.049611	4.021010
247.590229	5513.693716	7.704512	-0.049643	4.023812
247.982715	5521.738751	7.709517	-0.049721	4.026634
248.260738	5529.747124	7.714522	-0.049778	4.029440
248.236632	5537.825737	7.719526	-0.049779	4.032263
248.399772	5545.902168	7.724531	-0.049815	4.035087
248.625399	5553.887783	7.729536	-0.049862	4.037877
248.898405	5561.847512	7.734541	-0.049918	4.040658
249.069313	5569.808103	7.739546	-0.049955	4.043435
249.461887	5577.872725	7.744550	-0.050034	4.046250
249.710115	5585.868292	7.749555	-0.050085	4.049037
249.648273	5593.897364	7.754560	-0.050079	4.051829
249.864417	5601.957532	7.759565	-0.050125	4.054634
250.085830	5609.919772	7.764570	-0.050171	4.057402
250.322470	5617.940023	7.769574	-0.050220	4.060190
250.424511	5625.973066	7.774579	-0.050245	4.062978
250.621539	5633.978172	7.779584	-0.050287	4.065755
250.935112	5642.009481	7.784589	-0.050350	4.068542
250.994832	5650.000483	7.789594	-0.050367	4.071309
251.193746	5658.080885	7.794598	-0.050409	4.074107
251.329535	5666.082661	7.799603	-0.050440	4.076875
251.610992	5674.075255	7.804608	-0.050497	4.079640
251.817942	5682.105219	7.809613	-0.050541	4.082414
251.991559	5690.055111	7.814618	-0.050579	4.085159
252.116247	5698.144558	7.819622	-0.050607	4.087950
252.421053	5706.143009	7.824627	-0.050670	4.090709
252.542677	5714.187478	7.829632	-0.050697	4.093480
252.904195	5722.240247	7.834637	-0.050770	4.096256
253.046781	5730.201444	7.839642	-0.050802	4.098994
253.092627	5738.271618	7.844646	-0.050816	4.101768
253.305347	5746.217403	7.849651	-0.050861	4.104499
253.364860	5754.252490	7.854656	-0.050877	4.107256
253.471949	5762.280338	7.859661	-0.050902	4.110010
253.636893	5770.313341	7.864666	-0.050938	4.112765
254.013488	5778.399784	7.869670	-0.051014	4.115538
254.152828	5786.389951	7.874675	-0.051045	4.118274
254.353808	5794.374156	7.879680	-0.051088	4.121007
254.674393	5802.407933	7.884685	-0.051153	4.123756
254.976041	5810.410386	7.889690	-0.051214	4.126492
255.207052	5818.451887	7.894694	-0.051263	4.129239
255.425176	5826.448015	7.899699	-0.051309	4.131969
255.628085	5834.509622	7.904704	-0.051352	4.134719
255.784306	5842.564550	7.909709	-0.051386	4.137464
255.969776	5850.489007	7.914714	-0.051426	4.140163
256.033730	5858.557853	7.919718	-0.051443	4.142909
256.229012	5866.515522	7.924723	-0.051485	4.145616
256.552926	5874.586298	7.929728	-0.051550	4.148361
256.832392	5882.608856	7.934733	-0.051608	4.151087
256.783416	5890.659761	7.939738	-0.051604	4.153818
256.863010	5898.706151	7.944742	-0.051624	4.156546
257.272909	5906.671363	7.949747	-0.051706	4.159249
257.384627	5914.701540	7.954752	-0.051732	4.161969
257.809833	5922.679713	7.959757	-0.051816	4.164673
257.906119	5930.687783	7.964762	-0.051839	4.167382
258.178594	5938.701898	7.969766	-0.051896	4.170093
258.192592	5946.769404	7.974771	-0.051903	4.172817
258.283160	5954.787003	7.979776	-0.051926	4.175523
258.654897	5962.787055	7.984781	-0.052000	4.178225
258.979088	5970.763361	7.989786	-0.052066	4.180917
259.138107	5978.804824	7.994790	-0.052101	4.183627
259.222469	5986.813994	7.999795	-0.052122	4.186323
259.554548	5994.819793	8.004800	-0.052189	4.189019
259.729718	6002.910039	8.009805	-0.052227	4.191740
259.780003	6010.984326	8.014810	-0.052242	4.194453
260.082213	6018.998559	8.019814	-0.052303	4.197146
260.241108	6026.910672	8.024819	-0.052338	4.199802
260.440500	6034.906765	8.029824	-0.052380	4.202485
260.758952	6042.921301	8.034829	-0.052445	4.205173
260.965303	6050.905236	8.039834	-0.052489	4.207849
260.900865	6058.979747	8.044838	-0.052482	4.210550
261.294615	6066.992853	8.049843	-0.052561	4.213233
261.574655	6075.023871	8.054848	-0.052618	4.215920
261.700267	6083.066438	8.059853	-0.052647	4.218607
261.857764	6091.003802	8.064858	-0.052681	4.221257
262.215526	6099.059469	8.069862	-0.052753	4.223948
262.580957	6107.042445	8.074867	-0.052827	4.226612
262.625008	6115.078968	8.079872	-0.052840	4.229289
262.832499	6123.133902	8.084877	-0.052884	4.231973
263.052457	6131.182433	8.089882	-0.052930	4.234652
263.060678	6139.194042	8.094886	-0.052937	4.237316
263.076061	6147.142836	8.099891	-0.052945	4.239957
263.279377	6155.185586	8.104896	-0.052989	4.242630
263.545648	6163.228050	8.109901	-0.053043	4.245301
263.894405	6171.229247	8.114906	-0.053114	4.247957
264.203860	6179.239465	8.119910	-0.053177	4.250615
264.107594	6187.283358	8.124915	-0.053164	4.253278
264.290447	6195.289163	8.129920	-0.053203	4.255930
264.588630	6203.331058	8.134925	-0.053264	4.258592
264.840297	6211.309400	8.139930	-0.053316	4.261232
264.878895	6219.347358	8.144934	-0.053329	4.263888
265.039363	6227.386338	8.149939	-0.053364	4.266544
265.304887	6235.380453	8.154944	-0.053419	4.269184
265.233529	6243.433439	8.159949	-0.053411	4.271839
265.387275	6251.454607	8.164954	-0.053445	4.274483
265.692827	6259.501766	8.169958	-0.053507	4.277136
266.098640	6267.429228	8.174963	-0.053588	4.279748
266.194609	6275.483071	8.179968	-0.053611	4.282398
266.231239	6283.476862	8.184973	-0.053623	4.285026
266.388312	6291.520269	8.189978	-0.053658	4.287670
266.861266	6299.524224	8.194982	-0.053751	4.290302
266.844083	6307.593208	8.199987	-0.053753	4.292949
267.113996	6315.583427	8.204992	-0.053809	4.295571
267.330953	6323.620831	8.209997	-0.053854	4.298207
267.501290	6331.609966	8.215002	-0.053891	4.300825
267.750467	6339.626131	8.220006	-0.053943	4.303450
267.784817	6347.650166	8.225011	-0.053955	4.306075
267.789004	6355.653990	8.230016	-0.053961	4.308692
268.100010	6363.655035	8.235021	-0.054024	4.311308
268.410203	6371.701263	8.240026	-0.054087	4.313937
268.543870	6379.747705	8.245030	-0.054117	4.316564
268.499990	6387.689879	8.250035	-0.054115	4.319154
268.656709	6395.752365	8.255040	-0.054149	4.321782
268.985169	6403.728999	8.260045	-0.054216	4.324383
268.996067	6411.739200	8.265050	-0.054223	4.326990
269.344153	6419.804946	8.270054	-0.054293	4.329616
269.745775	6427.799730	8.275059	-0.054373	4.332218
269.920391	6435.830956	8.280064	-0.054411	4.334829
269.961272	6443.897651	8.285069	-0.054424	4.337449
270.191317	6451.833687	8.290074	-0.054472	4.340026
270.294839	6459.892553	8.295078	-0.054497	4.342640
270.496590	6467.843630	8.300083	-0.054539	4.345218
270.625514	6475.852968	8.305088	-0.054569	4.347814
271.022980	6483.919958	8.310093	-0.054648	4.350428
271.214125	6491.966869	8.315098	-0.054689	4.353032
271.620594	6500.043679	8.320102	-0.054770	4.355646
271.786386	6508.036174	8.325107	-0.054806	4.358230
272.016569	6515.962699	8.330112	-0.054854	4.360792
272.301920	6523.995558	8.335117	-0.054913	4.363386
272.365325	6531.944308	8.340122	-0.054930	4.365950
272.653420	6540.009108	8.345126	-0.054989	4.368552
272.733972	6548.051414	8.350131	-0.055009	4.371143
272.739236	6556.069756	8.355136	-0.055015	4.373725
273.010586	6564.128134	8.360141	-0.055071	4.376320
272.893136	6572.094012	8.365146	-0.055055	4.378881
273.182450	6580.132606	8.370150	-0.055114	4.381467
273.590686	6588.101217	8.375155	-0.055195	4.384029
273.648877	6596.102681	8.380160	-0.055211	4.386598
273.809000	6604.113083	8.385165	-0.055246	4.389169
273.841276	6612.190647	8.390170	-0.055258	4.391759
274.036582	6620.231489	8.395174	-0.055299	4.394337
274.144193	6628.282385	8.400179	-0.055325	4.396916
274.201394	6636.229552	8.405184	-0.055341	4.399460
274.614701	6644.276574	8.410189	-0.055423	4.402036
274.632076	6652.255207	8.415194	-0.055432	4.404587
274.766985	6660.283682	8.420198	-0.055462	4.407153
275.084262	6668.282007	8.425203	-0.055526	4.409709
275.225161	6676.320874	8.430208	-0.055558	4.412275
275.327282	6684.375798	8.435213	-0.055582	4.414845
275.786633	6692.396256	8.440218	-0.055673	4.417404
276.006121	6700.362080	8.445222	-0.055719	4.419943
275.924889	6708.399372	8.450227	-0.055709	4.422501
276.322398	6716.401617	8.455232	-0.055789	4.425050
276.688977	6724.453231	8.460237	-0.055862	4.427612
276.786385	6732.492474	8.465242	-0.055886	4.430167
277.044582	6740.536347	8.470246	-0.055939	4.432724
277.190340	6748.534235	8.475251	-0.055972	4.435263
277.351089	6756.545449	8.480256	-0.056007	4.437806
277.527752	6764.515838	8.485261	-0.056045	4.440334
277.669723	6772.517861	8.490266	-0.056077	4.442871
277.753913	6780.516319	8.495270	-0.056098	4.445405
277.902124	6788.591652	8.500275	-0.056131	4.447962
278.321102	6796.582789	8.505280	-0.056214	4.450491
278.630036	6804.651957	8.510285	-0.056277	4.453044
278.685847	6812.607076	8.515290	-0.056292	4.455558
278.890392	6820.658082	8.520294	-0.056336	4.458102
278.978377	6828.634854	8.525299	-0.056358	4.460620
279.194110	6836.670305	8.530304	-0.056403	4.463155
279.411159	6844.666825	8.535309	-0.056449	4.465677
279.736492	6852.683743	8.540314	-0.056515	4.468205
279.870002	6860.700244	8.545318	-0.056545	4.470730
279.943061	6868.757628	8.550323	-0.056564	4.473266
280.096585	6876.752365	8.555328	-0.056598	4.475781
280.584730	6884.802279	8.560333	-0.056694	4.478314
280.600129	6892.776657	8.565338	-0.056702	4.480819
280.655113	6900.810859	8.570343	-0.056718	4.483343
280.945684	6908.752104	8.575347	-0.056777	4.485836
281.192584	6916.812739	8.580352	-0.056828	4.488365
281.297981	6924.867215	8.585357	-0.056853	4.490890
281.370139	6932.882682	8.590362	-0.056872	4.493402
281.615559	6940.879402	8.595367	-0.056923	4.495907
281.786069	6948.901203	8.600371	-0.056960	4.498418
281.912420	6956.859994	8.605376	-0.056989	4.500908
282.258725	6964.925580	8.610381	-0.057059	4.503430
282.313840	6972.914881	8.615386	-0.057074	4.505926
282.472394	6980.976953	8.620391	-0.057109	4.508444
282.703170	6988.981097	8.625395	-0.057157	4.510943
282.906714	6997.041009	8.630400	-0.057200	4.513457
283.173053	7005.064051	8.635405	-0.057255	4.515959
283.124368	7013.009321	8.640410	-0.057252	4.518434
283.493631	7020.997668	8.645415	-0.057326	4.520923
283.642223	7029.053998	8.650419	-0.057359	4.523430
283.513073	7037.001889	8.655424	-0.057340	4.525902
283.918138	7045.075908	8.660429	-0.057421	4.528413
284.030143	7053.046464	8.665434	-0.057447	4.530890
284.134159	7061.129075	8.670439	-0.057471	4.533400
284.420354	7069.137913	8.675443	-0.057530	4.535886
284.599291	7077.102398	8.680448	-0.057569	4.538356
284.469707	7085.159207	8.685453	-0.057550	4.540854
284.507093	7093.101832	8.690458	-0.057562	4.543315
284.846467	7101.156562	8.695463	-0.057631	4.545810
285.078403	7109.196062	8.700467	-0.057679	4.548298
285.176421	7117.203161	8.705472	-0.057703	4.550775
285.682265	7125.263887	8.710477	-0.057802	4.553268
285.579490	7133.273431	8.715482	-0.057788	4.555743
285.833380	7141.305525	8.720487	-0.057841	4.558224
285.972548	7149.262469	8.725491	-0.057872	4.560680
286.101233	7157.280479	8.730496	-0.057901	4.563153
286.454919	7165.310512	8.735501	-0.057973	4.565629
286.675112	7173.344302	8.740506	-0.058019	4.568105
287.071439	7181.317339	8.745511	-0.058098	4.570561
287.246976	7189.392571	8.750515	-0.058136	4.573047
287.153731	7197.418845	8.755520	-0.058124	4.575516
287.397892	7205.505902	8.760525	-0.058175	4.578002
287.436948	7213.405604	8.765530	-0.058187	4.580430
287.701578	7221.430331	8.770535	-0.058242	4.582895
287.760656	7229.440285	8.775539	-0.058258	4.585354
288.243763	7237.462543	8.780544	-0.058353	4.587815
288.246200	7245.487368	8.785549	-0.058359	4.590276
288.378304	7253.516507	8.790554	-0.058389	4.592737
288.632183	7261.581640	8.795559	-0.058442	4.595207
288.832387	7269.600198	8.800563	-0.058484	4.597662
288.816350	7277.551560	8.805568	-0.058487	4.600095
288.940131	7285.630800	8.810573	-0.058515	4.602566
289.063730	7293.522360	8.815578	-0.058543	4.604978
289.283276	7301.583828	8.820583	-0.058589	4.607440
289.549094	7309.576125	8.825587	-0.058644	4.609881
289.638293	7317.632870	8.830592	-0.058666	4.612339
289.953814	7325.668758	8.835597	-0.058730	4.614790
289.957771	7333.685902	8.840602	-0.058736	4.617234
290.509707	7341.654162	8.845607	-0.058844	4.619661
290.593893	7349.721109	8.850611	-0.058865	4.622118
290.617791	7357.654740	8.855616	-0.058875	4.624532
291.014128	7365.759871	8.860621	-0.058954	4.626997
290.966345	7373.731566	8.865626	-0.058951	4.629421
291.175474	7381.767841	8.870631	-0.058995	4.631863
291.437905	7389.821993	8.875635	-0.059049	4.634308
291.778311	7397.813914	8.880640	-0.059118	4.636734
292.028388	7405.820117	8.885645	-0.059170	4.639162
292.028673	7413.786383	8.890650	-0.059175	4.641578
292.329577	7421.799264	8.895655	-0.059236	4.644006
292.653399	7429.836153	8.900659	-0.059302	4.646440
292.712717	7437.852470	8.905664	-0.059318	4.648867
292.921019	7445.907768	8.910669	-0.059362	4.651304
293.065758	7453.919567	8.915674	-0.059395	4.653726
293.274459	7461.943164	8.920679	-0.059439	4.656151
293.219290	7469.952061	8.925683	-0.059434	4.658571
293.631161	7477.877697	8.930688	-0.059516	4.660963
293.769914	7485.938470	8.935693	-0.059547	4.663395
293.821475	7493.895325	8.940698	-0.059562	4.665795
293.885319	7501.980685	8.945703	-0.059579	4.668233
294.261180	7510.022517	8.950707	-0.059654	4.670655
294.341956	7518.060544	8.955712	-0.059675	4.673076
294.576997	7526.178509	8.960717	-0.059724	4.675518
294.807679	7534.134702	8.965722	-0.059772	4.677911
295.057069	7542.015227	8.970727	-0.059824	4.680280
295.236690	7550.106127	8.975731	-0.059862	4.682712
295.175925	7558.014453	8.980736	-0.059856	4.685087
295.365192	7566.081603	8.985741	-0.059897	4.687509
295.337839	7574.039944	8.990746	-0.059897	4.689897
295.389375	7582.123762	8.995751	-0.059912	4.692321
295.653942	7590.173958	9.000755	-0.059967	4.694733
295.627795	7598.176958	9.005760	-0.059967	4.697131
295.793391	7606.180489	9.010765	-0.060003	4.699527
295.966834	7614.165291	9.015770	-0.060041	4.701916
296.440052	7622.206006	9.020775	-0.060134	4.704320
296.444891	7630.263411	9.025779	-0.060140	4.706729
296.627098	7638.199133	9.030784	-0.060180	4.709100
296.665381	7646.274517	9.035789	-0.060192	4.711512
296.624068	7654.284235	9.040794	-0.060190	4.713903
296.935395	7662.305734	9.045799	-0.060253	4.716295
297.324977	7670.312338	9.050803	-0.060331	4.718682
297.483164	7678.321792	9.055808	-0.060366	4.721068
297.722093	7686.339370	9.060813	-0.060415	4.723456
297.743394	7694.318898	9.065818	-0.060425	4.725832
298.037757	7702.389411	9.070823	-0.060485	4.728233
298.166259	7710.369901	9.075827	-0.060514	4.730606
298.115966	7718.437500	9.080832	-0.060510	4.733005
298.565077	7726.457171	9.085837	-0.060599	4.735386
298.607361	7734.437359	9.090842	-0.060612	4.737756
298.783877	7742.434748	9.095847	-0.060650	4.740130
298.859456	7750.490776	9.100851	-0.060670	4.742519
298.952012	7758.426854	9.105856	-0.060692	4.744873
298.987061	7766.557945	9.110861	-0.060704	4.747282
299.354283	7774.478174	9.115866	-0.060778	4.749627
299.579027	7782.551435	9.120871	-0.060825	4.752017
299.899760	7790.602684	9.125875	-0.060890	4.754398
299.950593	7798.595373	9.130880	-0.060905	4.756762
300.161232	7806.559377	9.135885	-0.060949	4.759116
300.282076	7814.542029	9.140890	-0.060977	4.761474
300.412675	7822.559491	9.145895	-0.061007	4.763842
300.710469	7830.592887	9.150899	-0.061067	4.766212
300.626714	7838.617521	9.155904	-0.061057	4.768580
300.815861	7846.614087	9.160909	-0.061098	4.770937
300.986676	7854.661034	9.165914	-0.061135	4.773309
301.180017	7862.709213	9.170919	-0.061176	4.775679
301.537176	7870.735319	9.175923	-0.061248	4.778041
301.265913	7878.686940	9.180928	-0.061203	4.780382
301.761460	7886.732826	9.185933	-0.061300	4.782747
301.733233	7894.716241	9.190938	-0.061300	4.785094
301.908568	7902.684500	9.195943	-0.061338	4.787435
302.154304	7910.748236	9.200947	-0.061389	4.789803
302.475483	7918.761984	9.205952	-0.061454	4.792154
302.479282	7926.876723	9.210957	-0.061460	4.794535
302.654915	7934.812049	9.215962	-0.061498	4.796861
302.912333	7942.816600	9.220967	-0.061552	4.799207
303.235240	7950.830557	9.225971	-0.061617	4.801553
303.053367	7958.827038	9.230976	-0.061588	4.803896
303.447325	7966.848104	9.235981	-0.061667	4.806242
303.467004	7974.857020	9.240986	-0.061676	4.808585
303.717803	7982.881468	9.245991	-0.061728	4.810930
303.968878	7990.333008	9.250995	-0.061780	4.813107
303.994423	7994.861888	9.256000	-0.061788	4.814430

304.237154	7997.489058	9.261005	-0.061835	4.815196
304.364479	7998.799718	9.266010	-0.061859	4.815578
304.346441	7999.283632	9.271015	-0.061856	4.815720
304.481941	8000.339091	9.276019	-0.061882	4.816027
304.439813	8000.273116	9.281024	-0.061874	4.816008
304.776155	8000.324186	9.286029	-0.061937	4.816021
304.934655	8000.302510	9.291034	-0.061967	4.816014
304.818906	8000.289707	9.296039	-0.061945	4.816011
304.918812	8000.294753	9.301043	-0.061964	4.816012
305.014107	8000.292231	9.306048	-0.061982	4.816010
305.025555	8000.345901	9.311053	-0.061984	4.816026
305.068142	8000.327447	9.316058	-0.061992	4.816020
304.870637	8000.267176	9.321063	-0.061955	4.816004
305.235451	8000.297388	9.326067	-0.062023	4.816011
305.234347	8000.321964	9.331072	-0.062023	4.816018
305.234080	8000.331589	9.336077	-0.062023	4.816021
305.293479	8000.315581	9.341082	-0.062034	4.816016
305.093085	8000.257395	9.346087	-0.061997	4.816000
305.263860	8000.299018	9.351091	-0.062029	4.816011
305.536525	8000.256984	9.356096	-0.062080	4.815997
305.658571	8000.268851	9.361101	-0.062103	4.816000
305.351445	8000.315614	9.366106	-0.062046	4.816015
305.528844	8000.350946	9.371111	-0.062079	4.816025
305.573995	8000.333607	9.376115	-0.062087	4.816020
305.352603	8000.286795	9.381120	-0.062046	4.816007
305.447180	8000.347335	9.386125	-0.062064	4.816024
305.588547	8000.347796	9.391130	-0.062090	4.816024
305.766403	8000.282644	9.396135	-0.062123	4.816004
305.574067	8000.340063	9.401139	-0.062088	4.816021
305.623914	8000.245838	9.406144	-0.062097	4.815994
305.765937	8000.276245	9.411149	-0.062124	4.816002
305.651842	8000.239952	9.416154	-0.062102	4.815992
305.679797	8000.240472	9.421159	-0.062108	4.815992
305.702423	8000.318937	9.426163	-0.062112	4.816015
305.818777	8000.280453	9.431168	-0.062134	4.816003
305.819925	8000.342488	9.436173	-0.062134	4.816021
305.861652	8000.337916	9.441178	-0.062142	4.816019
306.053800	8000.336101	9.446183	-0.062178	4.816018
305.864652	8000.275981	9.451187	-0.062143	4.816001
305.925910	8000.192655	9.456192	-0.062154	4.815976
306.075605	8000.321558	9.461197	-0.062182	4.816013
306.033218	8000.284440	9.466202	-0.062174	4.816003
306.139287	8000.272495	9.471207	-0.062194	4.815999
306.318921	8000.290763	9.476211	-0.062228	4.816003
306.186927	8000.346082	9.481216	-0.062203	4.816020
306.268454	8000.355068	9.486221	-0.062218	4.816022
306.280507	8000.355297	9.491226	-0.062221	4.816022
306.313514	8000.274660	9.496231	-0.062227	4.815998
306.157277	8000.302807	9.501235	-0.062198	4.816007
306.063765	8000.246578	9.506240	-0.062181	4.815991
306.383233	8000.388217	9.511245	-0.062240	4.816031
306.366627	8000.365469	9.516250	-0.062237	4.816025
306.185896	8000.325815	9.521255	-0.062204	4.816014
306.286883	8000.358678	9.526259	-0.062222	4.816023
306.268055	8000.319854	9.531264	-0.062219	4.816012
306.316963	8000.321828	9.536269	-0.062228	4.816012
306.221682	8000.292293	9.541274	-0.062211	4.816004
306.312160	8000.281131	9.546279	-0.062227	4.816000
306.331055	8000.355252	9.551283	-0.062231	4.816022
306.420595	8000.335520	9.556288	-0.062248	4.816015
306.657131	8000.353763	9.561293	-0.062292	4.816020
306.517480	8000.306309	9.566298	-0.062266	4.816006
306.606813	8000.263053	9.571303	-0.062283	4.815993
306.642234	8000.323580	9.576307	-0.062289	4.816011
306.631721	8000.229315	9.581312	-0.062288	4.815983
306.704921	8000.252047	9.586317	-0.062301	4.815990
306.761442	8000.287303	9.591322	-0.062312	4.816000
306.726065	8000.320873	9.596327	-0.062305	4.816010
306.511614	8000.341538	9.601331	-0.062266	4.816017
306.660729	8000.314346	9.606336	-0.062293	4.816008
306.740235	8000.414169	9.611341	-0.062308	4.816037
306.704513	8000.366482	9.616346	-0.062302	4.816023
306.620511	8000.332877	9.621351	-0.062286	4.816014
306.575987	8000.329930	9.626355	-0.062278	4.816013
306.636913	8000.281877	9.631360	-0.062289	4.815999
306.845044	8000.294254	9.636365	-0.062328	4.816001
306.774818	8000.291905	9.641370	-0.062315	4.816001
306.892867	8000.255591	9.646375	-0.062337	4.815990
306.770880	8000.341028	9.651379	-0.062315	4.816015
306.718557	8000.260964	9.656384	-0.062305	4.815992
306.989744	8000.334367	9.661389	-0.062356	4.816012
306.787767	8000.316773	9.666394	-0.062318	4.816008
306.636361	8000.341801	9.671399	-0.062290	4.816016
306.813693	8000.381410	9.676403	-0.062323	4.816027
306.945738	8000.313279	9.681408	-0.062348	4.816006
306.797450	8000.330881	9.686413	-0.062320	4.816012
306.757615	8000.335504	9.691418	-0.062313	4.816014
306.795420	8000.298787	9.696423	-0.062320	4.816003
306.947820	8000.343285	9.701427	-0.062348	4.816015
306.799352	8000.270010	9.706432	-0.062321	4.815994
306.952931	8000.292078	9.711437	-0.062349	4.816000
306.908302	8000.311580	9.716442	-0.062341	4.816006
306.975462	8000.308543	9.721447	-0.062354	4.816005
307.033689	8000.327794	9.726451	-0.062365	4.816010
307.056607	8000.195654	9.731456	-0.062369	4.815971
307.045035	8000.284185	9.736461	-0.062367	4.815997
307.141685	8000.306279	9.741466	-0.062385	4.816003
307.176339	8000.331512	9.746471	-0.062392	4.816010
307.021059	8000.355400	9.751475	-0.062363	4.816018
306.955096	8000.347784	9.756480	-0.062351	4.816016
307.108409	8000.281111	9.761485	-0.062379	4.815996
306.976923	8000.295814	9.766490	-0.062355	4.816001
307.094804	8000.337541	9.771495	-0.062377	4.816012
307.144745	8000.366262	9.776499	-0.062386	4.816020
307.178467	8000.238595	9.781504	-0.062393	4.815983
307.230677	8000.360370	9.786509	-0.062402	4.816018
307.219946	8000.313140	9.791514	-0.062401	4.816005
307.178533	8000.334840	9.796519	-0.062393	4.816011
307.322801	8000.352462	9.801523	-0.062420	4.816015
307.173472	8000.278101	9.806528	-0.062392	4.815995
307.284762	8000.323984	9.811533	-0.062413	4.816007
307.136907	8000.247512	9.816538	-0.062385	4.815986
307.071127	8000.254867	9.821543	-0.062373	4.815988
307.175976	8000.336980	9.826547	-0.062393	4.816012
307.278146	8000.316411	9.831552	-0.062412	4.816005
307.434820	8000.367403	9.836557	-0.062441	4.816019
307.190341	8000.352236	9.841562	-0.062396	4.816016
307.386640	8000.369743	9.846567	-0.062433	4.816020
307.330017	8000.372989	9.851571	-0.062422	4.816021
307.189928	8000.345838	9.856576	-0.062396	4.816014
307.391297	8000.359161	9.861581	-0.062434	4.816017
307.292685	8000.293214	9.866586	-0.062415	4.815998
307.339909	8000.289812	9.871591	-0.062424	4.815997
307.396976	8000.318663	9.876595	-0.062435	4.816005
307.251408	8000.225128	9.881600	-0.062408	4.815979
307.396301	8000.318667	9.886605	-0.062435	4.816005
307.457095	8000.322998	9.891610	-0.062446	4.816006
307.628544	8000.284455	9.896615	-0.062478	4.815994
307.395229	8000.328294	9.901619	-0.062435	4.816008
307.158934	8000.302586	9.906624	-0.062391	4.816002
307.281339	8000.271697	9.911629	-0.062414	4.815992
307.524144	8000.257983	9.916634	-0.062459	4.815987
307.513945	8000.298430	9.921639	-0.062457	4.815999
307.396468	8000.360431	9.926643	-0.062436	4.816017
307.498147	8000.270360	9.931648	-0.062455	4.815990
307.576628	8000.341300	9.936653	-0.062469	4.816011
307.298793	8000.290240	9.941658	-0.062418	4.815997
307.453293	8000.326224	9.946663	-0.062447	4.816007
307.459842	8000.394776	9.951667	-0.062448	4.816027
307.383654	8000.321756	9.956672	-0.062434	4.816006
307.610808	8000.348382	9.961677	-0.062476	4.816013
307.671767	8000.343094	9.966682	-0.062488	4.816011
307.435330	8000.372977	9.971687	-0.062444	4.816021
307.656418	8000.358865	9.976691	-0.062485	4.816015
307.557027	8000.373087	9.981696	-0.062466	4.816020
307.610026	8000.396519	9.986701	-0.062476	4.816027
307.514509	8000.322075	9.991706	-0.062459	4.816005
307.595830	8000.329989	9.996711	-0.062474	4.816007
307.751860	8000.362795	10.001715	-0.062503	4.816016
307.405061	8000.337197	10.006720	-0.062439	4.816010
307.572880	8000.407638	10.011725	-0.062470	4.816030
307.627611	8000.392614	10.016730	-0.062480	4.816025
307.797297	8000.303790	10.021735	-0.062512	4.815999
307.785609	8000.403012	10.026739	-0.062510	4.816028
307.881792	8000.326738	10.031744	-0.062528	4.816005
307.827983	8000.416635	10.036749	-0.062518	4.816031
307.738240	8000.346573	10.041754	-0.062501	4.816011
307.726077	8000.364533	10.046759	-0.062499	4.816017
307.763107	8000.391949	10.051763	-0.062506	4.816025
307.779322	8000.348420	10.056768	-0.062509	4.816012
307.731247	8000.387104	10.061773	-0.062500	4.816023
307.881701	8000.321448	10.066778	-0.062528	4.816003
307.750440	8000.309426	10.071783	-0.062504	4.816000
307.611283	8000.337886	10.076787	-0.062478	4.816010
307.687024	8000.353182	10.081792	-0.062492	4.816014
308.014912	8000.364551	10.086797	-0.062553	4.816015
307.800843	8000.380945	10.091802	-0.062514	4.816021
307.861641	8000.331820	10.096807	-0.062525	4.816006
307.980682	8000.393883	10.101811	-0.062547	4.816024
307.899487	8000.329323	10.106816	-0.062532	4.816005
307.835166	8000.338842	10.111821	-0.062520	4.816009
308.029080	8000.371275	10.116826	-0.062557	4.816017
308.007486	8000.291771	10.121831	-0.062553	4.815994
307.757693	8000.402662	10.126835	-0.062506	4.816028
307.741360	8000.376712	10.131840	-0.062503	4.816020
307.873264	8000.371656	10.136845	-0.062528	4.816018
307.885014	8000.391124	10.141850	-0.062530	4.816024
307.966672	8000.362694	10.146855	-0.062545	4.816015
307.794979	8000.345654	10.151859	-0.062514	4.816011
307.973538	8000.333970	10.156864	-0.062547	4.816006
308.096160	8000.435657	10.161869	-0.062570	4.816035
308.015953	8000.373253	10.166874	-0.062555	4.816018
307.968136	8000.315720	10.171879	-0.062546	4.816001
308.010121	8000.349641	10.176883	-0.062554	4.816011
307.891389	8000.328227	10.181888	-0.062532	4.816005
308.159579	8000.389819	10.186893	-0.062582	4.816022
308.027888	8000.343577	10.191898	-0.062558	4.816009
307.882645	8000.291741	10.196903	-0.062531	4.815995
308.141202	8000.365986	10.201907	-0.062579	4.816015
307.998500	8000.329163	10.206912	-0.062552	4.816005
307.966098	8000.373481	10.211917	-0.062546	4.816018
307.984083	8000.363127	10.216922	-0.062550	4.816015
308.045465	8000.341810	10.221927	-0.062561	4.816008
308.172829	8000.428617	10.226931	-0.062585	4.816033
308.037350	8000.356645	10.231936	-0.062560	4.816013
308.179800	8000.384926	10.236941	-0.062587	4.816020
308.102036	8000.395268	10.241946	-0.062572	4.816024
307.793746	8000.332956	10.246951	-0.062515	4.816007
307.971647	8000.412136	10.251955	-0.062548	4.816029
307.965797	8000.392792	10.256960	-0.062547	4.816024
307.962158	8000.370282	10.261965	-0.062547	4.816017
308.082950	8000.396027	10.266970	-0.062569	4.816024
307.952913	8000.348746	10.271975	-0.062545	4.816011
308.076916	8000.422661	10.276979	-0.062568	4.816032
308.034466	8000.358812	10.281984	-0.062560	4.816013
308.279546	8000.436018	10.286989	-0.062606	4.816035
308.263453	8000.401518	10.291994	-0.062603	4.816025
308.185622	8000.386199	10.296999	-0.062589	4.816020
308.048059	8000.430725	10.302003	-0.062563	4.816034
308.192084	8000.353191	10.307008	-0.062590	4.816011
308.187334	8000.401223	10.312013	-0.062589	4.816025
307.863839	8000.386743	10.317018	-0.062529	4.816022
307.994821	8000.390223	10.322023	-0.062554	4.816023
308.056327	8000.423434	10.327027	-0.062565	4.816032
308.011818	8000.356339	10.332032	-0.062557	4.816013
308.149900	8000.434789	10.337037	-0.062583	4.816035
308.259715	8000.385494	10.342042	-0.062603	4.816020
308.241400	8000.424724	10.347047	-0.062600	4.816031
308.259430	8000.423994	10.352051	-0.062603	4.816031
308.269260	8000.370725	10.357056	-0.062605	4.816015
308.109202	8000.412700	10.362061	-0.062576	4.816029
308.116847	8000.422471	10.367066	-0.062577	4.816031
308.270213	8000.415671	10.372071	-0.062606	4.816029
308.110068	8000.414879	10.377075	-0.062576	4.816029
308.121010	8000.373391	10.382080	-0.062578	4.816017
308.269754	8000.414618	10.387085	-0.062606	4.816028
308.097439	8000.372975	10.392090	-0.062574	4.816017
308.052317	8000.353980	10.397095	-0.062566	4.816012
308.278479	8000.409456	10.402099	-0.062608	4.816027
308.228211	8000.386090	10.407104	-0.062598	4.816020
308.145724	8000.405968	10.412109	-0.062583	4.816026
308.141850	8000.390937	10.417114	-0.062583	4.816022
308.209179	8000.339792	10.422119	-0.062595	4.816007
308.332778	8000.401940	10.427123	-0.062618	4.816024
308.208294	8000.407148	10.432128	-0.062595	4.816026
308.308069	8000.389742	10.437133	-0.062614	4.816021
308.295015	8000.415170	10.442138	-0.062611	4.816028
308.272482	8000.424387	10.447143	-0.062607	4.816031
308.387933	8000.433998	10.452147	-0.062629	4.816033
308.188962	8000.441046	10.457152	-0.062592	4.816036
308.155295	8000.457543	10.462157	-0.062586	4.816041
308.293530	8000.439774	10.467162	-0.062612	4.816035
308.445170	8000.424389	10.472167	-0.062640	4.816030
308.500984	8000.437182	10.477171	-0.062650	4.816034
308.470598	8000.414181	10.482176	-0.062645	4.816027
308.532231	8000.418527	10.487181	-0.062656	4.816028
308.535730	8000.415392	10.492186	-0.062657	4.816027
308.250096	8000.391983	10.497191	-0.062604	4.816022
308.179087	8000.411002	10.502195	-0.062591	4.816028
308.356730	8000.384334	10.507200	-0.062624	4.816019
308.484812	8000.430527	10.512205	-0.062648	4.816032
308.511696	8000.400024	10.517210	-0.062653	4.816023
308.511355	8000.431031	10.522215	-0.062653	4.816032
308.385042	8000.427652	10.527219	-0.062630	4.816031
308.229620	8000.409840	10.532224	-0.062601	4.816027
308.488558	8000.442397	10.537229	-0.062649	4.816035
308.458581	8000.422611	10.542234	-0.062644	4.816030
308.362360	8000.414438	10.547239	-0.062626	4.816028
308.413114	8000.435692	10.552243	-0.062635	4.816034
308.540706	8000.374961	10.557248	-0.062659	4.816015
308.490538	8000.360150	10.562253	-0.062650	4.816011
308.215679	8000.379705	10.567258	-0.062599	4.816018
308.238301	8000.361953	10.572263	-0.062603	4.816013
308.456485	8000.414076	10.577267	-0.062644	4.816027
308.297650	8000.398340	10.582272	-0.062614	4.816023
308.492627	8000.471420	10.587277	-0.062651	4.816044
308.445050	8000.435273	10.592282	-0.062642	4.816033
308.510118	8000.408678	10.597287	-0.062654	4.816025
308.454296	8000.445082	10.602291	-0.062644	4.816036
308.376341	8000.405170	10.607296	-0.062629	4.816025
308.720849	8000.436091	10.612301	-0.062694	4.816032
308.537685	8000.425253	10.617306	-0.062660	4.816030
308.394097	8000.409797	10.622311	-0.062633	4.816026
308.716760	8000.454216	10.627315	-0.062693	4.816037
308.564677	8000.425773	10.632320	-0.062665	4.816030
308.619079	8000.474891	10.637325	-0.062675	4.816044
308.461057	8000.451686	10.642330	-0.062646	4.816038
308.440042	8000.416026	10.647335	-0.062642	4.816028
308.519818	8000.453849	10.652339	-0.062657	4.816038
308.377251	8000.371055	10.657344	-0.062630	4.816015
308.379579	8000.388212	10.662349	-0.062631	4.816020
308.366135	8000.405080	10.667354	-0.062628	4.816025
308.668144	8000.384971	10.672359	-0.062685	4.816017
308.581051	8000.418663	10.677363	-0.062669	4.816028
308.416839	8000.382514	10.682368	-0.062638	4.816018
308.522968	8000.450757	10.687373	-0.062658	4.816037
308.615689	8000.405424	10.692378	-0.062675	4.816024
308.729385	8000.415002	10.697383	-0.062697	4.816026
308.693476	8000.428250	10.702387	-0.062690	4.816030
308.635375	8000.389772	10.707392	-0.062679	4.816019
308.583872	8000.412356	10.712397	-0.062670	4.816026
308.429158	8000.372105	10.717402	-0.062641	4.816015
308.570110	8000.423881	10.722407	-0.062667	4.816029
308.531626	8000.454188	10.727411	-0.062660	4.816038
308.514927	8000.383326	10.732416	-0.062657	4.816018
308.316513	8000.433150	10.737421	-0.062620	4.816033
308.376260	8000.422494	10.742426	-0.062632	4.816030
308.467094	8000.384610	10.747431	-0.062649	4.816018
308.473425	8000.447815	10.752435	-0.062650	4.816037
308.468537	8000.415658	10.757440	-0.062649	4.816027
308.696795	8000.403818	10.762445	-0.062692	4.816023
308.618276	8000.405593	10.767450	-0.062677	4.816024
308.432324	8000.345524	10.772455	-0.062642	4.816007
308.569990	8000.392962	10.777459	-0.062668	4.816020
308.593091	8000.388049	10.782464	-0.062673	4.816019
308.622951	8000.405711	10.787469	-0.062678	4.816024
308.581264	8000.445582	10.792474	-0.062671	4.816035
308.649072	8000.354887	10.797479	-0.062683	4.816009
308.804342	8000.440070	10.802483	-0.062712	4.816033
308.526878	8000.387943	10.807488	-0.062661	4.816019
308.634306	8000.384577	10.812493	-0.062681	4.816017
308.569910	8000.400510	10.817498	-0.062669	4.816022
308.477469	8000.412720	10.822503	-0.062652	4.816026
308.548858	8000.429007	10.827507	-0.062665	4.816031
308.531605	8000.419076	10.832512	-0.062662	4.816028
308.593020	8000.410589	10.837517	-0.062673	4.816025
308.583851	8000.418982	10.842522	-0.062672	4.816028
308.733048	8000.345818	10.847527	-0.062700	4.816005
308.519615	8000.404989	10.852531	-0.062660	4.816024
308.701846	8000.347400	10.857536	-0.062694	4.816006
308.700487	8000.377319	10.862541	-0.062694	4.816015
308.713936	8000.397888	10.867546	-0.062696	4.816021
308.683753	8000.414449	10.872551	-0.062691	4.816026
308.864109	8000.428459	10.877555	-0.062725	4.816029
308.651687	8000.393563	10.882560	-0.062685	4.816020
308.697561	8000.439317	10.887565	-0.062694	4.816033
308.716822	8000.446094	10.892570	-0.062697	4.816035
308.805920	8000.417801	10.897575	-0.062714	4.816026
308.928494	8000.466033	10.902579	-0.062737	4.816040
308.887675	8000.437493	10.907584	-0.062730	4.816031
308.764179	8000.467310	10.912589	-0.062707	4.816041
308.649812	8000.411761	10.917594	-0.062685	4.816025
308.797908	8000.390965	10.922599	-0.062713	4.816018
309.006444	8000.430083	10.927603	-0.062752	4.816029
308.967290	8000.397298	10.932608	-0.062745	4.816019
308.837347	8000.420581	10.937613	-0.062721	4.816027
308.822616	8000.438494	10.942618	-0.062718	4.816032
309.041365	8000.418996	10.947623	-0.062759	4.816025
309.015449	8000.444188	10.952627	-0.062754	4.816033
308.723438	8000.393932	10.957632	-0.062700	4.816020
308.819384	8000.407462	10.962637	-0.062718	4.816023
308.718739	8000.405623	10.967642	-0.062699	4.816023
308.710322	8000.363780	10.972647	-0.062698	4.816011
308.868815	8000.449022	10.977651	-0.062727	4.816035
308.657407	8000.393830	10.982656	-0.062688	4.816020
308.786799	8000.447532	10.987661	-0.062712	4.816035
308.868937	8000.424457	10.992666	-0.062727	4.816028
308.808597	8000.419081	10.997671	-0.062716	4.816026
308.696056	8000.433061	11.002675	-0.062695	4.816031
308.579780	8000.406345	11.007680	-0.062674	4.816024
308.705852	8000.420428	11.012685	-0.062697	4.816027
308.755666	8000.433111	11.017690	-0.062707	4.816031
308.672416	8000.424107	11.022695	-0.062691	4.816029
308.810061	8000.440540	11.027699	-0.062717	4.816033
308.880600	8000.355241	11.032704	-0.062730	4.816007
309.075626	8000.399457	11.037709	-0.062767	4.816019
308.932853	8000.412882	11.042714	-0.062740	4.816024
308.920705	8000.366693	11.047719	-0.062738	4.816010
309.003538	8000.451616	11.052723	-0.062753	4.816035
308.865017	8000.373171	11.057728	-0.062728	4.816013
308.933723	8000.347712	11.062733	-0.062741	4.816005
309.157146	8000.414901	11.067738	-0.062782	4.816023
309.096028	8000.452277	11.072743	-0.062771	4.816035
309.000316	8000.425938	11.077747	-0.062753	4.816027
308.828335	8000.408890	11.082752	-0.062721	4.816023
308.885379	8000.429190	11.087757	-0.062732	4.816029
308.845836	8000.432749	11.092762	-0.062725	4.816030
308.887339	8000.350125	11.097767	-0.062733	4.816006
309.049694	8000.447199	11.102771	-0.062763	4.816033
308.742522	8000.402010	11.107776	-0.062706	4.816022
308.942784	8000.409970	11.112781	-0.062743	4.816023
309.036440	8000.426666	11.117786	-0.062761	4.816027
308.805011	8000.395697	11.122791	-0.062718	4.816020
308.949694	8000.451819	11.127795	-0.062745	4.816035
309.022969	8000.363362	11.132800	-0.062758	4.816009
309.143170	8000.430796	11.137805	-0.062781	4.816028
309.133626	8000.463773	11.142810	-0.062779	4.816038
308.924232	8000.409687	11.147815	-0.062740	4.816023
309.152019	8000.450227	11.152819	-0.062783	4.816034
309.038867	8000.421429	11.157824	-0.062762	4.816026
308.970976	8000.447990	11.162829	-0.062749	4.816034
308.970612	8000.447991	11.167834	-0.062749	4.816034
308.980888	8000.447119	11.172839	-0.062751	4.816034
309.197826	8000.421172	11.177843	-0.062792	4.816025
309.097578	8000.433239	11.182848	-0.062773	4.816029
309.172739	8000.404690	11.187853	-0.062787	4.816020
309.233519	8000.405814	11.192858	-0.062799	4.816020
309.258375	8000.430870	11.197863	-0.062803	4.816027
309.331983	8000.441851	11.202867	-0.062817	4.816030
309.132517	8000.447820	11.207872	-0.062780	4.816033
309.081381	8000.447959	11.212877	-0.062771	4.816033
309.123800	8000.425224	11.217882	-0.062779	4.816026
308.995821	8000.358733	11.222887	-0.062755	4.816008
309.090783	8000.406459	11.227891	-0.062773	4.816021
308.896834	8000.385800	11.232896	-0.062737	4.816016
309.005325	8000.445534	11.237901	-0.062757	4.816033
308.912910	8000.420325	11.242906	-0.062740	4.816026
309.032721	8000.404356	11.247911	-0.062762	4.816021
309.276058	8000.463359	11.252915	-0.062808	4.816037
309.207235	8000.464242	11.257920	-0.062795	4.816037
309.101744	8000.417408	11.262925	-0.062775	4.816024
309.096160	8000.456873	11.267930	-0.062774	4.816036
309.097008	8000.432306	11.272935	-0.062775	4.816029
309.203003	8000.441744	11.277939	-0.062794	4.816031
308.974957	8000.417252	11.282944	-0.062752	4.816025
309.107575	8000.454977	11.287949	-0.062777	4.816035
309.035874	8000.439769	11.292954	-0.062763	4.816031
309.080991	8000.447021	11.297959	-0.062772	4.816033
309.315933	8000.456688	11.302963	-0.062816	4.816035
309.148944	8000.435454	11.307968	-0.062785	4.816029
308.995693	8000.463655	11.312973	-0.062756	4.816038
309.141757	8000.447100	11.317978	-0.062784	4.816033
309.026836	8000.437514	11.322983	-0.062762	4.816030
309.121555	8000.479889	11.327987	-0.062780	4.816042
308.941553	8000.426342	11.332992	-0.062747	4.816028
309.088557	8000.440810	11.337997	-0.062774	4.816031
309.108432	8000.459358	11.343002	-0.062778	4.816036
308.996422	8000.373916	11.348007	-0.062757	4.816012
309.366041	8000.453412	11.353011	-0.062826	4.816033
309.167866	8000.442298	11.358016	-0.062789	4.816031
309.204511	8000.437633	11.363021	-0.062796	4.816030
309.134693	8000.460950	11.368026	-0.062783	4.816037
309.218053	8000.425068	11.373031	-0.062799	4.816026
309.402619	8000.433810	11.378035	-0.062833	4.816027
309.275449	8000.398339	11.383040	-0.062810	4.816018
309.341460	8000.439118	11.388045	-0.062822	4.816029
309.122377	8000.428690	11.393050	-0.062781	4.816027
309.116149	8000.382609	11.398055	-0.062780	4.816014
309.136451	8000.406512	11.403059	-0.062784	4.816021
309.162617	8000.379202	11.408064	-0.062789	4.816013
309.099856	8000.399441	11.413069	-0.062777	4.816019
309.194100	8000.323130	11.418074	-0.062795	4.815996
309.223896	8000.351484	11.423079	-0.062801	4.816004
309.252304	8000.424717	11.428083	-0.062806	4.816025
309.107945	8000.397484	11.433088	-0.062779	4.816018
309.224613	8000.403910	11.438093	-0.062801	4.816020
309.235738	8000.422298	11.443098	-0.062803	4.816025
309.177794	8000.338917	11.448103	-0.062792	4.816001
309.240377	8000.408501	11.453107	-0.062804	4.816021
309.518304	8000.457447	11.458112	-0.062856	4.816034
309.431499	8000.438755	11.463117	-0.062840	4.816029
309.234926	8000.411632	11.468122	-0.062803	4.816022
309.207255	8000.376919	11.473127	-0.062798	4.816012
309.228679	8000.439332	11.478131	-0.062802	4.816030
309.059343	8000.399880	11.483136	-0.062771	4.816019
309.130377	8000.465343	11.488141	-0.062784	4.816038
309.351318	8000.448023	11.493146	-0.062825	4.816032
309.309152	8000.422666	11.498151	-0.062818	4.816025
309.391462	8000.492613	11.503155	-0.062833	4.816045
309.075069	8000.469706	11.508160	-0.062774	4.816040
309.180068	8000.456673	11.513165	-0.062794	4.816035
309.147198	8000.455008	11.518170	-0.062788	4.816035
309.342033	8000.448971	11.523175	-0.062824	4.816032
309.519848	8000.500356	11.528179	-0.062857	4.816046
309.288928	8000.436251	11.533184	-0.062815	4.816029
309.515985	8000.453258	11.538189	-0.062857	4.816032
309.482033	8000.461196	11.543194	-0.062851	4.816035
309.167059	8000.392341	11.548199	-0.062792	4.816016
309.342138	8000.476820	11.553203	-0.062825	4.816040
309.540450	8000.435563	11.558208	-0.062862	4.816027
309.548110	8000.463511	11.563213	-0.062863	4.816035
309.320797	8000.446516	11.568218	-0.062821	4.816031
309.348250	8000.395707	11.573223	-0.062826	4.816016
309.483982	8000.434559	11.578227	-0.062852	4.816027
309.423310	8000.382133	11.583232	-0.062840	4.816012
309.390047	8000.343040	11.588237	-0.062834	4.816001
309.448555	8000.439279	11.593242	-0.062845	4.816029
309.424502	8000.455952	11.598247	-0.062841	4.816034
309.405576	8000.482342	11.603251	-0.062837	4.816041
309.288427	8000.435294	11.608256	-0.062816	4.816028
309.393464	8000.463960	11.613261	-0.062835	4.816036
309.366118	8000.433529	11.618266	-0.062830	4.816027
309.367584	8000.449602	11.623271	-0.062831	4.816032
309.446181	8000.487405	11.628275	-0.062845	4.816043
309.322970	8000.406032	11.633280	-0.062822	4.816020
309.578316	8000.469533	11.638285	-0.062870	4.816037
309.379726	8000.457342	11.643290	-0.062833	4.816034
309.166215	8000.426701	11.648295	-0.062794	4.816026
309.368452	8000.461428	11.653299	-0.062831	4.816035
309.385210	8000.367656	11.658304	-0.062834	4.816008
309.587642	8000.459053	11.663309	-0.062872	4.816034
309.551112	8000.440214	11.668314	-0.062866	4.816028
309.483434	8000.390867	11.673319	-0.062853	4.816014
309.624570	8000.472586	11.678323	-0.062879	4.816037
309.577864	8000.419346	11.683328	-0.062871	4.816022
309.418176	8000.400385	11.688333	-0.062841	4.816017
309.642666	8000.469735	11.693338	-0.062883	4.816036
309.450442	8000.427723	11.698343	-0.062847	4.816025
309.381117	8000.437150	11.703347	-0.062834	4.816028
309.376876	8000.422112	11.708352	-0.062834	4.816024
309.449568	8000.455530	11.713357	-0.062847	4.816033
309.326140	8000.428681	11.718362	-0.062824	4.816026
309.334256	8000.401040	11.723367	-0.062826	4.816018
309.506637	8000.440565	11.728371	-0.062858	4.816029
309.276162	8000.436341	11.733376	-0.062815	4.816029
309.397235	8000.479201	11.738381	-0.062838	4.816040
309.431271	8000.463796	11.743386	-0.062845	4.816036
309.175932	8000.370376	11.748391	-0.062797	4.816010
309.305327	8000.490368	11.753395	-0.062821	4.816044
309.353491	8000.450632	11.758400	-0.062830	4.816032
309.495907	8000.451116	11.763405	-0.062857	4.816032
309.332282	8000.426737	11.768410	-0.062826	4.816025
309.301964	8000.421912	11.773415	-0.062821	4.816024
309.438519	8000.442603	11.778419	-0.062846	4.816030
309.534986	8000.449728	11.783424	-0.062864	4.816031
309.560916	8000.459835	11.788429	-0.062869	4.816034
309.507961	8000.455663	11.793434	-0.062860	4.816033
309.458366	8000.389541	11.798439	-0.062850	4.816014
309.688211	8000.463265	11.803443	-0.062893	4.816034
309.629290	8000.441877	11.808448	-0.062882	4.816028
309.680145	8000.464203	11.813453	-0.062892	4.816035
309.522553	8000.490185	11.818458	-0.062863	4.816043
309.560339	8000.458812	11.823463	-0.062870	4.816034
309.572961	8000.521064	11.828467	-0.062872	4.816052
309.380815	8000.471570	11.833472	-0.062837	4.816038
309.437792	8000.443756	11.838477	-0.062847	4.816030
309.662016	8000.476749	11.843482	-0.062889	4.816038
309.507714	8000.453609	11.848487	-0.062860	4.816032
309.313323	8000.446841	11.853491	-0.062824	4.816031
309.424377	8000.425366	11.858496	-0.062845	4.816025
309.420050	8000.434917	11.863501	-0.062844	4.816027
309.424080	8000.459591	11.868506	-0.062845	4.816035
309.288923	8000.407935	11.873511	-0.062820	4.816020
309.587834	8000.479720	11.878515	-0.062876	4.816040
309.530960	8000.434848	11.883520	-0.062865	4.816027
309.566872	8000.452622	11.888525	-0.062872	4.816032
309.609321	8000.451271	11.893530	-0.062880	4.816031
309.647627	8000.465882	11.898535	-0.062887	4.816035
309.524064	8000.499974	11.903539	-0.062864	4.816046
309.536874	8000.486318	11.908544	-0.062867	4.816042
309.763021	8000.486201	11.913549	-0.062909	4.816040
309.584404	8000.478653	11.918554	-0.062876	4.816039
309.538724	8000.409395	11.923559	-0.062867	4.816019
309.670317	8000.463140	11.928563	-0.062892	4.816034
309.541185	8000.434048	11.933568	-0.062868	4.816026
309.583399	8000.417724	11.938573	-0.062876	4.816021
309.801309	8000.450601	11.943578	-0.062917	4.816030
309.846880	8000.455722	11.948583	-0.062925	4.816031
309.820911	8000.503367	11.953587	-0.062921	4.816045
309.645291	8000.447761	11.958592	-0.062888	4.816030
309.654336	8000.491771	11.963597	-0.062890	4.816043
309.751491	8000.526708	11.968602	-0.062908	4.816052
309.776550	8000.479063	11.973607	-0.062913	4.816038
309.722157	8000.488764	11.978611	-0.062903	4.816041
309.765220	8000.491701	11.983616	-0.062911	4.816042
309.695282	8000.459419	11.988621	-0.062898	4.816033
309.654399	8000.508928	11.993626	-0.062890	4.816048
309.533969	8000.441505	11.998631	-0.062868	4.816029
309.571168	8000.495655	12.003635	-0.062875	4.816044
309.639985	8000.468059	12.008640	-0.062888	4.816036
309.676466	8000.502951	12.013645	-0.062895	4.816046
309.543524	8000.491964	12.018650	-0.062870	4.816043
309.703319	8000.452139	12.023655	-0.062900	4.816031
309.696208	8000.456293	12.028659	-0.062899	4.816032
309.740581	8000.421833	12.033664	-0.062907	4.816022
309.512999	8000.369550	12.038669	-0.062865	4.816008
309.728870	8000.453710	12.043674	-0.062905	4.816031
309.537686	8000.428824	12.048679	-0.062869	4.816025
309.694004	8000.454155	12.053683	-0.062899	4.816031
309.614568	8000.440944	12.058688	-0.062884	4.816028
309.639207	8000.475618	12.063693	-0.062889	4.816038
309.895653	8000.501719	12.068698	-0.062936	4.816044
309.527679	8000.455410	12.073703	-0.062868	4.816033
309.765754	8000.475828	12.078707	-0.062912	4.816037
309.798697	8000.458265	12.083712	-0.062919	4.816032
309.742127	8000.424089	12.088717	-0.062908	4.816022
309.636161	8000.468127	12.093722	-0.062888	4.816036
309.591154	8000.438440	12.098727	-0.062880	4.816027
309.701599	8000.478967	12.103731	-0.062901	4.816039
309.672550	8000.463473	12.108736	-0.062895	4.816034
309.696612	8000.453231	12.113741	-0.062900	4.816031
309.799044	8000.455120	12.118746	-0.062919	4.816031
309.586798	8000.437332	12.123751	-0.062880	4.816027
309.685567	8000.468021	12.128755	-0.062898	4.816035
309.492014	8000.416363	12.133760	-0.062862	4.816021
309.462924	8000.435082	12.138765	-0.062857	4.816027
309.771355	8000.458929	12.143770	-0.062914	4.816032
309.769090	8000.478141	12.148775	-0.062914	4.816038
309.718182	8000.480422	12.153779	-0.062905	4.816039
309.511437	8000.410345	12.158784	-0.062866	4.816020
309.506493	8000.371772	12.163789	-0.062865	4.816008
309.789053	8000.436842	12.168794	-0.062918	4.816026
309.588423	8000.431028	12.173799	-0.062881	4.816025
309.754259	8000.454395	12.178803	-0.062912	4.816031
309.768127	8000.415098	12.183808	-0.062914	4.816020
309.668568	8000.402587	12.188813	-0.062896	4.816016
309.683185	8000.478775	12.193818	-0.062899	4.816039
309.825092	8000.445037	12.198823	-0.062925	4.816028
309.735356	8000.417737	12.203827	-0.062909	4.816020
309.629110	8000.362335	12.208832	-0.062889	4.816005
309.775934	8000.443089	12.213837	-0.062916	4.816028
309.884458	8000.485719	12.218842	-0.062937	4.816040
309.457497	8000.436190	12.223847	-0.062857	4.816027
309.617101	8000.435920	12.228851	-0.062887	4.816026
309.577323	8000.409538	12.233856	-0.062880	4.816019
309.606633	8000.389770	12.238861	-0.062885	4.816013
309.717522	8000.445273	12.243866	-0.062906	4.816029
309.557164	8000.400639	12.248871	-0.062876	4.816016
309.757037	8000.459914	12.253875	-0.062914	4.816033
309.704879	8000.430096	12.258880	-0.062904	4.816024
309.600076	8000.411074	12.263885	-0.062884	4.816019
309.747058	8000.476862	12.268890	-0.062912	4.816038
309.549310	8000.418711	12.273895	-0.062875	4.816022
309.757587	8000.396883	12.278899	-0.062914	4.816014
309.680209	8000.431823	12.283904	-0.062900	4.816025
309.821102	8000.440833	12.288909	-0.062926	4.816027
309.682723	8000.463960	12.293914	-0.062900	4.816034
309.567835	8000.422299	12.298919	-0.062879	4.816023
309.564152	8000.457523	12.303923	-0.062878	4.816033
309.542849	8000.444310	12.308928	-0.062875	4.816029
309.560382	8000.458539	12.313933	-0.062878	4.816033
309.753885	8000.473861	12.318938	-0.062914	4.816037
309.526261	8000.448306	12.323943	-0.062872	4.816030
309.552483	8000.487286	12.328947	-0.062877	4.816042
309.620392	8000.457535	12.333952	-0.062889	4.816033
309.708408	8000.453813	12.338957	-0.062906	4.816031
309.838175	8000.475450	12.343962	-0.062930	4.816037
309.773120	8000.395143	12.348967	-0.062918	4.816014
309.783505	8000.490500	12.353971	-0.062920	4.816041
309.794185	8000.449006	12.358976	-0.062922	4.816029
309.696968	8000.425845	12.363981	-0.062904	4.816023
309.908925	8000.490689	12.368986	-0.062944	4.816041
309.882338	8000.475240	12.373991	-0.062939	4.816036
309.902179	8000.480959	12.378995	-0.062943	4.816038
309.708155	8000.451743	12.384000	-0.062907	4.816030
309.672209	8000.438261	12.389005	-0.062900	4.816027
309.693327	8000.468594	12.394010	-0.062904	4.816035
309.852242	8000.462967	12.399015	-0.062934	4.816033
309.886874	8000.517071	12.404019	-0.062940	4.816049
309.602564	8000.466952	12.409024	-0.062887	4.816035
309.656690	8000.452985	12.414029	-0.062898	4.816031
309.892964	8000.501169	12.419034	-0.062942	4.816044
309.580561	8000.453742	12.424039	-0.062883	4.816032
309.562975	8000.494056	12.429043	-0.062880	4.816044
309.631868	8000.460046	12.434048	-0.062893	4.816033
309.701846	8000.490208	12.439053	-0.062906	4.816042
309.735949	8000.463043	12.444058	-0.062913	4.816034
309.574607	8000.415183	12.449063	-0.062883	4.816020
309.714534	8000.460528	12.454067	-0.062909	4.816033
309.725585	8000.477846	12.459072	-0.062911	4.816038
309.592958	8000.444412	12.464077	-0.062886	4.816029
309.694772	8000.420629	12.469082	-0.062905	4.816021
309.775981	8000.400745	12.474087	-0.062921	4.816015
309.649140	8000.458298	12.479091	-0.062897	4.816033
309.600294	8000.440303	12.484096	-0.062888	4.816028
309.754214	8000.432445	12.489101	-0.062917	4.816025
309.725269	8000.469343	12.494106	-0.062912	4.816035
309.610692	8000.443726	12.499111	-0.062890	4.816029
309.832573	8000.449946	12.504115	-0.062932	4.816029
309.739908	8000.451460	12.509120	-0.062915	4.816030
309.687768	8000.461203	12.514125	-0.062905	4.816033
309.804735	8000.449459	12.519130	-0.062927	4.816029
309.721538	8000.395550	12.524135	-0.062911	4.816014
309.820430	8000.428380	12.529139	-0.062930	4.816023
309.866322	8000.498728	12.534144	-0.062939	4.816043
309.834122	8000.432924	12.539149	-0.062933	4.816024
309.696252	8000.430401	12.544154	-0.062907	4.816024
309.616774	8000.339139	12.549159	-0.062892	4.815998
309.745755	8000.368244	12.554163	-0.062916	4.816006
309.787568	8000.436379	12.559168	-0.062924	4.816025
309.739039	8000.364930	12.564173	-0.062915	4.816005
309.726008	8000.421365	12.569178	-0.062913	4.816021
309.800233	8000.390661	12.574183	-0.062927	4.816012
309.837915	8000.441612	12.579187	-0.062934	4.816027
309.846241	8000.436428	12.584192	-0.062936	4.816025
309.924258	8000.445353	12.589197	-0.062950	4.816027
309.920683	8000.472025	12.594202	-0.062950	4.816035
309.874864	8000.442323	12.599207	-0.062941	4.816027
309.819473	8000.453076	12.604211	-0.062931	4.816030
309.874919	8000.443410	12.609216	-0.062941	4.816027
309.897717	8000.405346	12.614221	-0.062946	4.816016
309.923715	8000.411177	12.619226	-0.062951	4.816017
309.801398	8000.411078	12.624231	-0.062928	4.816018
309.891106	8000.470469	12.629235	-0.062945	4.816035
309.756833	8000.443421	12.634240	-0.062920	4.816028
309.842334	8000.439653	12.639245	-0.062936	4.816026
309.915063	8000.469864	12.644250	-0.062949	4.816035
309.777485	8000.413887	12.649255	-0.062924	4.816019
309.780527	8000.428919	12.654259	-0.062925	4.816023
310.026808	8000.454834	12.659264	-0.062970	4.816030
309.703698	8000.412556	12.664269	-0.062910	4.816019
309.810505	8000.451947	12.669274	-0.062930	4.816030
309.809273	8000.415580	12.674279	-0.062930	4.816019
309.789999	8000.466556	12.679283	-0.062927	4.816034
309.749300	8000.426256	12.684288	-0.062919	4.816023
309.787715	8000.462253	12.689293	-0.062926	4.816033
309.939004	8000.465039	12.694298	-0.062955	4.816033
309.745552	8000.421935	12.699303	-0.062919	4.816021
309.839485	8000.441844	12.704307	-0.062936	4.816027
309.951056	8000.452455	12.709312	-0.062957	4.816029
309.932467	8000.457467	12.714317	-0.062954	4.816031
309.911224	8000.479539	12.719322	-0.062950	4.816037
309.859889	8000.446528	12.724327	-0.062940	4.816028
309.932562	8000.470324	12.729331	-0.062954	4.816035
309.983881	8000.464859	12.734336	-0.062964	4.816033
309.938496	8000.415920	12.739341	-0.062955	4.816019
309.995047	8000.450112	12.744346	-0.062966	4.816028
309.973078	8000.440094	12.749351	-0.062962	4.816025
310.036870	8000.448758	12.754355	-0.062974	4.816028
310.004030	8000.423571	12.759360	-0.062968	4.816020
309.895624	8000.431212	12.764365	-0.062948	4.816023
309.976934	8000.472273	12.769370	-0.062963	4.816035
310.080032	8000.455998	12.774375	-0.062982	4.816030
310.085847	8000.509573	12.779379	-0.062983	4.816045
309.934445	8000.466171	12.784384	-0.062955	4.816033
309.948818	8000.484619	12.789389	-0.062958	4.816039
310.010743	8000.472934	12.794394	-0.062970	4.816035
309.858046	8000.417748	12.799399	-0.062941	4.816020
310.039966	8000.366568	12.804403	-0.062975	4.816004
310.004034	8000.401200	12.809408	-0.062969	4.816014
310.051570	8000.413842	12.814413	-0.062978	4.816017
309.905021	8000.450719	12.819418	-0.062950	4.816029
309.872525	8000.424470	12.824423	-0.062944	4.816021
310.010850	8000.418464	12.829427	-0.062970	4.816019
309.962745	8000.398344	12.834432	-0.062961	4.816013
310.071760	8000.368278	12.839437	-0.062982	4.816004
310.067134	8000.448390	12.844442	-0.062981	4.816027
310.026371	8000.403813	12.849447	-0.062973	4.816015
309.974823	8000.446712	12.854451	-0.062964	4.816027
309.795851	8000.465886	12.859456	-0.062931	4.816034
309.781505	8000.411102	12.864461	-0.062928	4.816018
309.925732	8000.410551	12.869466	-0.062955	4.816017
309.737692	8000.408176	12.874471	-0.062920	4.816017
310.011682	8000.391831	12.879475	-0.062971	4.816011
309.938484	8000.415086	12.884480	-0.062958	4.816018
309.821845	8000.484588	12.889485	-0.062936	4.816039
309.894454	8000.496622	12.894490	-0.062950	4.816042
309.914175	8000.431771	12.899495	-0.062953	4.816023
309.977563	8000.466089	12.904499	-0.062965	4.816033
310.037332	8000.449018	12.909504	-0.062977	4.816028
310.088209	8000.449960	12.914509	-0.062986	4.816028
310.074100	8000.484993	12.919514	-0.062984	4.816038
309.945724	8000.449498	12.924519	-0.062960	4.816028
310.055349	8000.484665	12.929523	-0.062980	4.816038
310.169038	8000.451477	12.934528	-0.063001	4.816028
310.038556	8000.486511	12.939533	-0.062977	4.816039
309.952200	8000.496694	12.944538	-0.062961	4.816042
309.828375	8000.426000	12.949543	-0.062938	4.816022
309.943886	8000.455929	12.954547	-0.062960	4.816030
310.062579	8000.460255	12.959552	-0.062982	4.816031
310.070280	8000.476442	12.964557	-0.062984	4.816035
309.964475	8000.474507	12.969562	-0.062964	4.816035
309.871948	8000.428980	12.974567	-0.062947	4.816023
310.242517	8000.446485	12.979571	-0.063016	4.816026
310.083915	8000.424335	12.984576	-0.062986	4.816020
309.849705	8000.454256	12.989581	-0.062943	4.816030
310.221891	8000.488898	12.994586	-0.063012	4.816038
310.066432	8000.414415	12.999591	-0.062983	4.816017
310.012934	8000.490423	13.004595	-0.062974	4.816040
310.012847	8000.463700	13.009600	-0.062974	4.816032
309.992121	8000.465465	13.014605	-0.062970	4.816033
309.936921	8000.504020	13.019610	-0.062960	4.816044
309.972719	8000.426634	13.024615	-0.062966	4.816021
310.165092	8000.480428	13.029619	-0.063002	4.816036
310.018390	8000.441389	13.034624	-0.062975	4.816025
309.970824	8000.372095	13.039629	-0.062966	4.816005
310.128198	8000.455183	13.044634	-0.062996	4.816029
310.017980	8000.426437	13.049639	-0.062975	4.816021
309.997745	8000.460288	13.054643	-0.062972	4.816031
310.093040	8000.442800	13.059648	-0.062989	4.816025
309.983941	8000.461120	13.064653	-0.062969	4.816031
310.047542	8000.501856	13.069658	-0.062981	4.816043
309.897117	8000.456334	13.074663	-0.062953	4.816030
310.114417	8000.483855	13.079667	-0.062994	4.816037
310.159422	8000.448337	13.084672	-0.063002	4.816027
310.066798	8000.438090	13.089677	-0.062985	4.816024
310.038415	8000.501729	13.094682	-0.062980	4.816043
310.101990	8000.460137	13.099687	-0.062992	4.816030
310.031120	8000.484504	13.104691	-0.062979	4.816038
309.912186	8000.468429	13.109696	-0.062957	4.816034
309.972255	8000.478093	13.114701	-0.062968	4.816036
310.097770	8000.501791	13.119706	-0.062991	4.816043
309.935294	8000.485984	13.124711	-0.062961	4.816039
310.062197	8000.464801	13.129715	-0.062985	4.816032
310.174011	8000.443340	13.134720	-0.063006	4.816025
310.029674	8000.439628	13.139725	-0.062979	4.816025
309.914330	8000.461040	13.144730	-0.062958	4.816032
309.921406	8000.438725	13.149735	-0.062959	4.816025
309.933534	8000.432541	13.154739	-0.062961	4.816023
309.967739	8000.451354	13.159744	-0.062968	4.816029
310.101603	8000.439921	13.164749	-0.062993	4.816025
310.130703	8000.494992	13.169754	-0.062998	4.816040
309.837645	8000.422259	13.174759	-0.062944	4.816021
310.068425	8000.453235	13.179763	-0.062987	4.816029
310.066527	8000.487423	13.184768	-0.062987	4.816039
309.962290	8000.449164	13.189773	-0.062967	4.816028
310.051736	8000.456161	13.194778	-0.062984	4.816030
310.075413	8000.436289	13.199783	-0.062988	4.816024
309.994079	8000.463672	13.204787	-0.062973	4.816032
310.006286	8000.442520	13.209792	-0.062976	4.816026
310.016229	8000.394597	13.214797	-0.062978	4.816012
310.095312	8000.450586	13.219802	-0.062992	4.816028
310.077768	8000.381844	13.224807	-0.062989	4.816008
310.320977	8000.499654	13.229811	-0.063035	4.816041
310.129722	8000.450173	13.234816	-0.062999	4.816027
310.035267	8000.431340	13.239821	-0.062982	4.816022
310.206768	8000.505065	13.244826	-0.063014	4.816043
310.200316	8000.508162	13.249831	-0.063013	4.816044
310.261634	8000.512504	13.254835	-0.063024	4.816045
310.023802	8000.447200	13.259840	-0.062980	4.816027
310.194281	8000.483484	13.264845	-0.063012	4.816037
310.337572	8000.510715	13.269850	-0.063038	4.816044
309.988921	8000.475452	13.274855	-0.062974	4.816035
310.275025	8000.501029	13.279859	-0.063027	4.816041
310.159834	8000.486091	13.284864	-0.063006	4.816038
310.089207	8000.485871	13.289869	-0.062992	4.816038
310.034582	8000.509468	13.294874	-0.062982	4.816045
310.265498	8000.464534	13.299879	-0.063025	4.816031
310.171840	8000.472445	13.304883	-0.063008	4.816034
310.044123	8000.473315	13.309888	-0.062984	4.816035
310.057723	8000.466088	13.314893	-0.062987	4.816032
310.245170	8000.489854	13.319898	-0.063022	4.816038
310.352598	8000.449067	13.324903	-0.063042	4.816026
310.274064	8000.522477	13.329907	-0.063028	4.816048
310.261208	8000.483758	13.334912	-0.063025	4.816036
310.090177	8000.479555	13.339917	-0.062993	4.816036
310.194181	8000.511411	13.344922	-0.063013	4.816045
310.051663	8000.482072	13.349927	-0.062986	4.816037
310.103988	8000.503356	13.354931	-0.062996	4.816043
310.225098	8000.468166	13.359936	-0.063019	4.816032
310.315667	8000.491222	13.364941	-0.063036	4.816038
310.492243	8000.522273	13.369946	-0.063069	4.816046
310.161199	8000.478778	13.374951	-0.063007	4.816035
310.147860	8000.518102	13.379955	-0.063005	4.816047
310.127063	8000.495275	13.384960	-0.063001	4.816040
310.151934	8000.486117	13.389965	-0.063006	4.816038
310.277951	8000.493785	13.394970	-0.063029	4.816039
310.084548	8000.496657	13.399975	-0.062993	4.816041
310.175210	8000.500468	13.404979	-0.063010	4.816042
310.018707	8000.499740	13.409984	-0.062981	4.816042
310.004571	8000.452444	13.414989	-0.062979	4.816029
310.180451	8000.472790	13.419994	-0.063012	4.816034
310.211048	8000.474429	13.424999	-0.063017	4.816034
310.178343	8000.493082	13.430003	-0.063011	4.816040
310.096882	8000.504424	13.435008	-0.062996	4.816043
310.114448	8000.479094	13.440013	-0.063000	4.816036
310.099283	8000.486308	13.445018	-0.062997	4.816038
310.097452	8000.433892	13.450023	-0.062997	4.816023
310.293133	8000.485608	13.455027	-0.063033	4.816037
310.273178	8000.476696	13.460032	-0.063030	4.816034
310.096410	8000.479873	13.465037	-0.062997	4.816036
310.280692	8000.502511	13.470042	-0.063031	4.816042
310.110319	8000.459830	13.475047	-0.062999	4.816030
310.042394	8000.436137	13.480051	-0.062987	4.816024
310.212219	8000.449956	13.485056	-0.063019	4.816027
310.286490	8000.436360	13.490061	-0.063032	4.816022
310.284734	8000.467342	13.495066	-0.063032	4.816031
310.077637	8000.467824	13.500071	-0.062994	4.816033
310.250310	8000.498802	13.505075	-0.063026	4.816041
310.255915	8000.485014	13.510080	-0.063027	4.816037
310.068994	8000.462343	13.515085	-0.062992	4.816031
310.280576	8000.484414	13.520090	-0.063032	4.816036
310.312633	8000.428343	13.525095	-0.063038	4.816020
310.414803	8000.490103	13.530099	-0.063057	4.816037
310.331362	8000.483233	13.535104	-0.063042	4.816036
310.233034	8000.440805	13.540109	-0.063023	4.816024
310.315048	8000.482949	13.545114	-0.063039	4.816036
310.094273	8000.431858	13.550119	-0.062998	4.816022
310.431655	8000.462654	13.555123	-0.063061	4.816029
310.140917	8000.475499	13.560128	-0.063007	4.816035
310.245474	8000.438936	13.565133	-0.063026	4.816023
310.591857	8000.465621	13.570138	-0.063091	4.816029
310.476531	8000.466718	13.575143	-0.063069	4.816030
310.306031	8000.497809	13.580147	-0.063038	4.816040
310.259846	8000.468101	13.585152	-0.063029	4.816032
310.365856	8000.473263	13.590157	-0.063049	4.816033
310.273355	8000.480126	13.595162	-0.063032	4.816035
310.121466	8000.440992	13.600167	-0.063004	4.816025
310.383900	8000.470412	13.605171	-0.063053	4.816032
310.428497	8000.454132	13.610176	-0.063061	4.816027
310.416723	8000.420778	13.615181	-0.063059	4.816017
310.521845	8000.492216	13.620186	-0.063078	4.816037
310.382329	8000.481107	13.625191	-0.063053	4.816035
310.378024	8000.506697	13.630195	-0.063052	4.816042
310.356718	8000.509522	13.635200	-0.063048	4.816043
310.201899	8000.476749	13.640205	-0.063019	4.816035
310.233544	8000.515829	13.645210	-0.063025	4.816046
310.221437	8000.517753	13.650215	-0.063023	4.816046
310.256072	8000.473491	13.655219	-0.063030	4.816033
310.290138	8000.442049	13.660224	-0.063036	4.816024
310.055109	8000.421703	13.665229	-0.062992	4.816019
310.343402	8000.472981	13.670234	-0.063046	4.816033
310.455766	8000.459015	13.675239	-0.063067	4.816028
310.252079	8000.495912	13.680243	-0.063029	4.816040
310.299113	8000.464707	13.685248	-0.063038	4.816030
310.566307	8000.384087	13.690253	-0.063088	4.816005
310.494164	8000.495037	13.695258	-0.063075	4.816038
310.189541	8000.470204	13.700263	-0.063018	4.816033
310.412845	8000.511736	13.705267	-0.063060	4.816044
310.199274	8000.490714	13.710272	-0.063020	4.816039
310.231488	8000.434646	13.715277	-0.063026	4.816022
310.349518	8000.515943	13.720282	-0.063048	4.816045
310.241407	8000.431637	13.725287	-0.063028	4.816021
310.222758	8000.513631	13.730291	-0.063025	4.816045
310.395641	8000.499707	13.735296	-0.063057	4.816040
310.379989	8000.443829	13.740301	-0.063054	4.816024
310.480790	8000.485249	13.745306	-0.063073	4.816035
310.367376	8000.448960	13.750311	-0.063052	4.816025
310.489647	8000.471528	13.755315	-0.063075	4.816031
310.494590	8000.482319	13.760320	-0.063076	4.816035
310.269728	8000.438637	13.765325	-0.063034	4.816023
310.371445	8000.465105	13.770330	-0.063053	4.816030
310.268597	8000.419387	13.775335	-0.063034	4.816017
310.335337	8000.461250	13.780339	-0.063046	4.816029
310.401244	8000.457123	13.785344	-0.063059	4.816028
310.331830	8000.409880	13.790349	-0.063046	4.816014
310.419094	8000.463882	13.795354	-0.063062	4.816030
310.270412	8000.436568	13.800359	-0.063035	4.816022
310.288120	8000.542753	13.805363	-0.063038	4.816053
310.420866	8000.499223	13.810368	-0.063063	4.816040
310.366885	8000.481132	13.815373	-0.063053	4.816035
310.291827	8000.481900	13.820378	-0.063039	4.816035
310.310680	8000.455525	13.825383	-0.063043	4.816028
310.397574	8000.488136	13.830387	-0.063059	4.816037
310.310705	8000.450195	13.835392	-0.063043	4.816026
310.495114	8000.451452	13.840397	-0.063077	4.816025
310.537530	8000.489662	13.845402	-0.063085	4.816036
310.176337	8000.414607	13.850407	-0.063018	4.816016
310.322375	8000.487864	13.855411	-0.063045	4.816037
310.276860	8000.506282	13.860416	-0.063037	4.816043
310.179482	8000.484187	13.865421	-0.063019	4.816037
310.300873	8000.503532	13.870426	-0.063041	4.816042
310.345893	8000.478706	13.875431	-0.063050	4.816034
310.544845	8000.516583	13.880435	-0.063087	4.816044
310.282017	8000.496795	13.885440	-0.063038	4.816040
310.225840	8000.485079	13.890445	-0.063028	4.816037
310.376878	8000.499622	13.895450	-0.063056	4.816040
310.213073	8000.414293	13.900455	-0.063026	4.816016
310.162554	8000.447588	13.905459	-0.063016	4.816026
310.353871	8000.488532	13.910464	-0.063052	4.816037
310.361823	8000.448056	13.915469	-0.063054	4.816025
310.318751	8000.501803	13.920474	-0.063046	4.816041
310.363902	8000.447042	13.925479	-0.063054	4.816025
310.600847	8000.490963	13.930483	-0.063098	4.816036
310.430171	8000.512428	13.935488	-0.063067	4.816044
310.333647	8000.486071	13.940493	-0.063049	4.816036
310.475370	8000.519689	13.945498	-0.063075	4.816045
310.512580	8000.473336	13.950503	-0.063082	4.816032
310.391431	8000.506402	13.955507	-0.063060	4.816042
310.300812	8000.454493	13.960512	-0.063043	4.816027
310.178642	8000.427666	13.965517	-0.063020	4.816020
310.205388	8000.496594	13.970522	-0.063025	4.816040
310.245449	8000.473816	13.975527	-0.063033	4.816033
310.231958	8000.489614	13.980531	-0.063030	4.816038
310.420734	8000.500574	13.985536	-0.063066	4.816040
310.405176	8000.507781	13.990541	-0.063063	4.816042
310.681692	8000.503246	13.995546	-0.063114	4.816040
310.442909	8000.499937	14.000551	-0.063070	4.816040
310.357148	8000.482331	14.005555	-0.063054	4.816035
310.278202	8000.493720	14.010560	-0.063040	4.816039
310.309630	8000.460091	14.015565	-0.063045	4.816029
310.204303	8000.463510	14.020570	-0.063026	4.816030
310.252265	8000.451569	14.025575	-0.063035	4.816027
310.383671	8000.424053	14.030579	-0.063059	4.816018
310.323260	8000.461443	14.035584	-0.063048	4.816029
310.261028	8000.428232	14.040589	-0.063037	4.816020
310.228775	8000.489661	14.045594	-0.063031	4.816038
310.190565	8000.486829	14.050599	-0.063024	4.816037
310.301668	8000.481394	14.055603	-0.063045	4.816035
310.258918	8000.480616	14.060608	-0.063037	4.816035
310.227137	8000.437273	14.065613	-0.063031	4.816023
310.395910	8000.497049	14.070618	-0.063062	4.816039
310.343292	8000.486467	14.075623	-0.063053	4.816036
310.416967	8000.493175	14.080627	-0.063067	4.816038
310.290680	8000.459856	14.085632	-0.063043	4.816029
310.229533	8000.438427	14.090637	-0.063032	4.816023
310.463255	8000.519711	14.095642	-0.063075	4.816045
310.364512	8000.483690	14.100647	-0.063057	4.816035
310.253493	8000.489144	14.105651	-0.063036	4.816038
310.340903	8000.471512	14.110656	-0.063053	4.816032
310.382578	8000.466939	14.115661	-0.063061	4.816030
310.420469	8000.487958	14.120666	-0.063068	4.816036
310.309185	8000.457054	14.125671	-0.063047	4.816028
310.370402	8000.482778	14.130675	-0.063059	4.816035
310.203805	8000.484003	14.135680	-0.063028	4.816036
309.918961	8000.399659	14.140685	-0.062975	4.816013
310.283547	8000.487622	14.145690	-0.063043	4.816037
310.318664	8000.500037	14.150695	-0.063049	4.816040
310.433791	8000.475429	14.155699	-0.063071	4.816033
310.323195	8000.502274	14.160704	-0.063050	4.816041
310.388155	8000.431839	14.165709	-0.063063	4.816020
310.426760	8000.503124	14.170714	-0.063070	4.816041
310.387708	8000.471408	14.175719	-0.063063	4.816032
310.460979	8000.466346	14.180723	-0.063076	4.816030
310.443438	8000.456409	14.185728	-0.063073	4.816027
310.344339	8000.402206	14.190733	-0.063055	4.816012
310.330342	8000.487494	14.195738	-0.063052	4.816037
310.484718	8000.453984	14.200743	-0.063081	4.816026
310.216430	8000.422335	14.205747	-0.063031	4.816018
310.426987	8000.467909	14.210752	-0.063071	4.816030
310.369795	8000.439067	14.215757	-0.063060	4.816022
310.392979	8000.515415	14.220762	-0.063064	4.816045
310.277208	8000.479082	14.225767	-0.063043	4.816035
310.274786	8000.445900	14.230771	-0.063042	4.816025
310.448480	8000.469414	14.235776	-0.063075	4.816031
310.335317	8000.428852	14.240781	-0.063054	4.816020
310.545511	8000.525742	14.245786	-0.063093	4.816047
310.413520	8000.490180	14.250791	-0.063069	4.816037
310.451381	8000.504783	14.255795	-0.063076	4.816041
310.531602	7999.307721	14.260800	-0.063090	4.815691

310.318223	7996.125599	14.265805	-0.063048	4.814763
310.455883	7990.658263	14.270810	-0.063070	4.813165
310.482802	7983.955907	14.275815	-0.063071	4.811206
310.490645	7976.663375	14.280819	-0.063068	4.809074
310.336455	7969.010525	14.285824	-0.063034	4.806837
310.076315	7961.171727	14.290829	-0.062981	4.804544
310.255841	7953.391256	14.295834	-0.063009	4.802266
310.142433	7945.373929	14.300839	-0.062983	4.799918
309.943896	7937.434766	14.305843	-0.062941	4.797592
310.026836	7929.427570	14.310848	-0.062951	4.795244
310.050785	7921.380740	14.315853	-0.062951	4.792884
309.993568	7913.409939	14.320858	-0.062935	4.790545
309.852004	7905.383244	14.325863	-0.062903	4.788188
309.820345	7897.370803	14.330867	-0.062892	4.785835
309.830914	7889.441571	14.335872	-0.062889	4.783504
309.610062	7881.395873	14.340877	-0.062843	4.781139
309.728594	7873.444301	14.345882	-0.062860	4.778799
309.609826	7865.431509	14.350887	-0.062833	4.776441
309.609170	7857.386330	14.355891	-0.062827	4.774072
309.738684	7849.388378	14.360896	-0.062846	4.771715
309.630101	7841.354890	14.365901	-0.062821	4.769347
309.698958	7833.389356	14.370906	-0.062829	4.766998
309.492785	7825.348757	14.375911	-0.062785	4.764626
309.584459	7817.413651	14.380915	-0.062797	4.762283
309.530601	7809.358910	14.385920	-0.062782	4.759904
309.397693	7801.351517	14.390925	-0.062752	4.757538
309.297359	7793.379214	14.395930	-0.062728	4.755181
309.312643	7785.307971	14.400935	-0.062726	4.752793
309.214580	7777.315252	14.405939	-0.062703	4.750428
309.060912	7769.311095	14.410944	-0.062669	4.748059
308.928206	7761.291249	14.415949	-0.062639	4.745683
309.052916	7753.386055	14.420954	-0.062657	4.743339
308.894813	7745.286593	14.425959	-0.062622	4.740938
308.722394	7737.347869	14.430963	-0.062585	4.738583
308.883052	7729.299322	14.435968	-0.062610	4.736193
308.859990	7721.323070	14.440973	-0.062601	4.733824
308.761742	7713.331068	14.445978	-0.062577	4.731449
308.917108	7705.312361	14.450983	-0.062601	4.729065
308.605121	7697.316658	14.455987	-0.062538	4.726687
308.769922	7689.281997	14.460992	-0.062563	4.724296
308.706369	7681.354806	14.465997	-0.062546	4.721935
308.954464	7673.369888	14.471002	-0.062587	4.719556
308.504678	7665.312693	14.476007	-0.062499	4.717156
308.597818	7657.295554	14.481011	-0.062511	4.714765
308.752148	7649.318621	14.486016	-0.062534	4.712384
308.387449	7641.232996	14.491021	-0.062461	4.709971
308.556600	7633.310298	14.496026	-0.062488	4.707605
308.473330	7625.268044	14.501031	-0.062467	4.705202
308.355434	7617.313144	14.506035	-0.062440	4.702824
308.256716	7609.290494	14.511040	-0.062416	4.700424
308.191235	7601.337976	14.516045	-0.062399	4.698044
308.365982	7593.313367	14.521050	-0.062427	4.695641
308.055841	7585.306530	14.526055	-0.062364	4.693243
307.966332	7577.257787	14.531059	-0.062342	4.690830
307.899189	7569.256073	14.536064	-0.062324	4.688431
307.891314	7561.274546	14.541069	-0.062318	4.686036
307.982264	7553.329037	14.546074	-0.062329	4.683650
307.955288	7545.310836	14.551079	-0.062319	4.681242
308.133435	7537.310691	14.556083	-0.062347	4.678837
308.023433	7529.315736	14.561088	-0.062322	4.676434
307.780059	7521.177763	14.566093	-0.062271	4.673986
307.698105	7513.156157	14.571098	-0.062251	4.671572
307.852428	7505.166130	14.576103	-0.062274	4.669166
307.700660	7497.210425	14.581107	-0.062241	4.666769
307.901715	7489.244383	14.586112	-0.062273	4.664367
307.679137	7481.242712	14.591117	-0.062227	4.661954
307.482909	7473.227840	14.596122	-0.062185	4.659536
307.449322	7465.264594	14.601127	-0.062174	4.657131
307.541871	7457.221399	14.606131	-0.062186	4.654702
307.280430	7449.252931	14.611136	-0.062132	4.652294
307.189336	7441.155321	14.616141	-0.062110	4.649845
307.283603	7433.257827	14.621146	-0.062122	4.647455
307.029799	7425.173151	14.626151	-0.062070	4.645008
306.966317	7417.278088	14.631155	-0.062053	4.642617
307.025588	7409.244439	14.636160	-0.062059	4.640183
307.160504	7401.245127	14.641165	-0.062079	4.637757
307.050782	7393.237774	14.646170	-0.062053	4.635328
306.893457	7385.170752	14.651175	-0.062019	4.632880
306.889016	7377.166102	14.656179	-0.062013	4.630449
306.798577	7369.203422	14.661184	-0.061991	4.628030
306.727950	7361.134116	14.666189	-0.061973	4.625577
306.836070	7353.200934	14.671194	-0.061988	4.623164
306.790682	7345.181242	14.676199	-0.061974	4.620724
306.559494	7337.221791	14.681203	-0.061926	4.618300
306.703031	7329.229445	14.686208	-0.061947	4.615865
306.587160	7321.159911	14.691213	-0.061921	4.613406
306.444146	7313.173499	14.696218	-0.061889	4.610970
306.500313	7305.195737	14.701223	-0.061894	4.608536
306.415571	7297.154533	14.706227	-0.061873	4.606081
306.360644	7289.188193	14.711232	-0.061858	4.603648
306.091584	7281.143200	14.716237	-0.061803	4.601190
306.229421	7273.192689	14.721242	-0.061823	4.598758
306.108510	7265.186041	14.726247	-0.061796	4.596309
306.025098	7257.154155	14.731251	-0.061775	4.593850
306.108299	7249.095019	14.736256	-0.061785	4.591382
306.061856	7241.114571	14.741261	-0.061772	4.588937
305.961855	7233.129262	14.746266	-0.061748	4.586488
306.058110	7225.127802	14.751271	-0.061761	4.584034
306.076798	7217.169301	14.756275	-0.061759	4.581591
305.980196	7209.156207	14.761280	-0.061736	4.579130
305.857769	7201.110927	14.766285	-0.061708	4.576658
305.695020	7193.134067	14.771290	-0.061673	4.574206
305.603502	7185.090416	14.776295	-0.061650	4.571732
305.670222	7177.091453	14.781299	-0.061658	4.569270
305.761847	7169.118021	14.786304	-0.061670	4.566815
305.538025	7161.104949	14.791309	-0.061623	4.564346
305.555538	7153.182822	14.796314	-0.061621	4.561904
305.477750	7145.138682	14.801319	-0.061601	4.559423
305.718240	7137.155743	14.806323	-0.061641	4.556960
305.477645	7129.136994	14.811328	-0.061591	4.554484
305.384843	7121.101031	14.816333	-0.061569	4.552001
305.567363	7113.116044	14.821338	-0.061597	4.549533
305.579244	7105.096565	14.826343	-0.061594	4.547053
305.401879	7097.058967	14.831347	-0.061556	4.544566
305.198041	7089.129786	14.836352	-0.061513	4.542111
305.428388	7081.088341	14.841357	-0.061551	4.539620
305.497063	7073.159671	14.846362	-0.061559	4.537163
305.144529	7065.131487	14.851367	-0.061488	4.534672
305.023492	7057.115829	14.856371	-0.061460	4.532185
305.090868	7049.064501	14.861376	-0.061468	4.529686
304.941677	7041.106114	14.866381	-0.061435	4.527213
305.037583	7033.099634	14.871386	-0.061447	4.524725
304.878243	7025.159144	14.876391	-0.061413	4.522256
304.838842	7017.113042	14.881395	-0.061400	4.519752
304.898921	7009.185133	14.886400	-0.061406	4.517284
304.999820	7001.061892	14.891405	-0.061420	4.514754
304.842759	6993.016888	14.896410	-0.061385	4.512246
304.684734	6985.052502	14.901415	-0.061351	4.509763
304.728172	6977.036218	14.906419	-0.061354	4.507262
304.651436	6969.043192	14.911424	-0.061334	4.504766
304.476896	6961.074306	14.916429	-0.061297	4.502277
304.380748	6953.088366	14.921434	-0.061274	4.499781
304.498523	6945.091343	14.926439	-0.061291	4.497280
304.498227	6937.047755	14.931443	-0.061285	4.494764
304.368092	6929.086463	14.936448	-0.061256	4.492271
304.425434	6921.027508	14.941453	-0.061262	4.489747
304.448610	6913.066963	14.946458	-0.061261	4.487252
304.231546	6905.039207	14.951463	-0.061215	4.484734
304.047361	6897.071478	14.956467	-0.061176	4.482234
304.311381	6889.072525	14.961472	-0.061220	4.479723
304.179581	6881.055678	14.966477	-0.061190	4.477205
304.098347	6873.052869	14.971482	-0.061170	4.474689
304.044551	6865.002733	14.976487	-0.061155	4.472158
304.167222	6856.976327	14.981491	-0.061172	4.469633
304.201959	6849.043510	14.986496	-0.061174	4.467135
304.149757	6840.987179	14.991501	-0.061159	4.464598
304.031752	6833.085658	14.996506	-0.061132	4.462107
304.146698	6825.058519	15.001511	-0.061148	4.459576
303.884889	6817.037893	15.006515	-0.061094	4.457044
303.907605	6809.066333	15.011520	-0.061093	4.454527
303.633193	6801.008664	15.016525	-0.061037	4.451981
303.728077	6793.039495	15.021530	-0.061050	4.449463
303.784145	6785.000244	15.026535	-0.061055	4.446920
303.712729	6777.014389	15.031539	-0.061036	4.444393
303.620529	6769.038286	15.036544	-0.061014	4.441867
303.625448	6760.986790	15.041549	-0.061010	4.439317
303.717992	6753.064901	15.046554	-0.061022	4.436806
303.457443	6745.006167	15.051559	-0.060968	4.434249
303.299446	6736.944027	15.056563	-0.060934	4.431690
303.324832	6728.980616	15.061568	-0.060933	4.429162
303.164983	6720.938671	15.066573	-0.060899	4.426606
303.226594	6712.999669	15.071578	-0.060905	4.424082
303.156778	6704.998240	15.076583	-0.060887	4.421537
303.280850	6697.005706	15.081587	-0.060905	4.418994
303.222364	6689.000625	15.086592	-0.060889	4.416444
303.111992	6680.969572	15.091597	-0.060863	4.413885
303.207197	6672.946213	15.096602	-0.060876	4.411327
302.927541	6664.949454	15.101607	-0.060818	4.408775
302.858225	6656.962228	15.106611	-0.060800	4.406225
302.994802	6649.027462	15.111616	-0.060821	4.403692
302.685541	6641.001281	15.116621	-0.060758	4.401126
302.749307	6633.023109	15.121626	-0.060765	4.398575
302.812184	6624.992003	15.126631	-0.060771	4.396006
302.824611	6616.980979	15.131635	-0.060768	4.393441
302.656259	6608.943355	15.136640	-0.060732	4.390866
302.489769	6600.979635	15.141645	-0.060696	4.388313
302.667123	6592.944069	15.146650	-0.060724	4.385737
302.441822	6584.986804	15.151655	-0.060677	4.383183
302.536461	6576.967783	15.156659	-0.060689	4.380608
302.567204	6568.993369	15.161664	-0.060690	4.378047
302.350721	6561.009321	15.166669	-0.060644	4.375479
302.402080	6552.990569	15.171674	-0.060649	4.372901
302.220924	6544.958224	15.176679	-0.060610	4.370315
302.099140	6537.006254	15.181683	-0.060582	4.367753
302.229810	6528.992571	15.186688	-0.060601	4.365172
302.012838	6520.998475	15.191693	-0.060556	4.362594
301.909822	6512.983933	15.196698	-0.060531	4.360008
301.830117	6505.030821	15.201703	-0.060512	4.357440
301.849329	6496.967555	15.206707	-0.060510	4.354836
301.783238	6488.897174	15.211712	-0.060492	4.352228
301.727192	6480.861399	15.216717	-0.060477	4.349629
301.752304	6472.938888	15.221722	-0.060476	4.347066
301.663714	6464.926817	15.226727	-0.060455	4.344471
301.629579	6456.970551	15.231731	-0.060443	4.341894
301.572422	6448.967483	15.236736	-0.060428	4.339299
301.387657	6441.000620	15.241741	-0.060388	4.336714
301.492049	6432.942424	15.246746	-0.060402	4.334100
301.564932	6424.941592	15.251751	-0.060411	4.331502
301.458892	6416.945331	15.256755	-0.060386	4.328904
301.427688	6408.952388	15.261760	-0.060375	4.326305
301.296068	6400.936604	15.266765	-0.060345	4.323697
301.145909	6392.970214	15.271770	-0.060312	4.321102
301.104844	6384.972834	15.276775	-0.060299	4.318497
301.109751	6376.969748	15.281779	-0.060295	4.315889
301.183820	6368.974806	15.286784	-0.060304	4.313283
300.915390	6360.862013	15.291789	-0.060249	4.310634
301.109821	6352.924869	15.296794	-0.060280	4.308044
301.055880	6344.938678	15.301799	-0.060265	4.305434
300.767927	6336.947292	15.306803	-0.060206	4.302820
301.022801	6328.934381	15.311808	-0.060248	4.300201
300.963072	6320.932431	15.316813	-0.060232	4.297582
300.827571	6312.947606	15.321818	-0.060202	4.294966
300.585029	6304.931127	15.326823	-0.060151	4.292337
300.864233	6296.890401	15.331827	-0.060198	4.289703
300.849021	6288.939417	15.336832	-0.060190	4.287094
300.626594	6280.902163	15.341837	-0.060144	4.284454
300.813187	6272.943824	15.346842	-0.060173	4.281841
300.766038	6264.933221	15.351847	-0.060159	4.279207
300.449290	6256.935056	15.356851	-0.060095	4.276574
300.474090	6248.929820	15.361856	-0.060095	4.273940
300.471113	6240.836373	15.366861	-0.060089	4.271275
300.543637	6232.923235	15.371866	-0.060097	4.268668
300.219611	6224.879049	15.376871	-0.060032	4.266013
300.291816	6216.900029	15.381875	-0.060040	4.263381
300.327140	6208.904161	15.386880	-0.060042	4.260742
300.143035	6200.928304	15.391885	-0.060002	4.258105
300.519554	6192.883527	15.396890	-0.060067	4.255450
300.264595	6184.889286	15.401895	-0.060015	4.252803
300.019820	6176.897036	15.406899	-0.059964	4.250156
300.042429	6168.918844	15.411904	-0.059963	4.247514
299.953335	6160.856278	15.416909	-0.059941	4.244842
299.903213	6152.931451	15.421914	-0.059927	4.242214
299.807480	6144.931894	15.426919	-0.059904	4.239559
299.842029	6136.932916	15.431923	-0.059905	4.236904
299.859569	6128.973234	15.436928	-0.059903	4.234260
299.690750	6120.866859	15.441933	-0.059867	4.231563
299.670080	6112.903303	15.446938	-0.059858	4.228914
299.487972	6104.895812	15.451943	-0.059819	4.226248
299.611703	6096.933585	15.456947	-0.059837	4.223597
299.642429	6088.948978	15.461952	-0.059837	4.220936
299.573132	6080.941367	15.466957	-0.059819	4.218266
299.379006	6072.917194	15.471962	-0.059778	4.215586
299.308585	6064.938567	15.476967	-0.059760	4.212922
299.382102	6056.876760	15.481971	-0.059768	4.210229
299.501630	6048.932634	15.486976	-0.059785	4.207574
299.392745	6040.903189	15.491981	-0.059760	4.204887
299.411737	6032.970234	15.496986	-0.059758	4.202232
299.258965	6024.971952	15.501991	-0.059725	4.199551
299.139536	6016.968532	15.506995	-0.059697	4.196868
299.160509	6008.903687	15.512000	-0.059696	4.194163
299.005075	6000.835471	15.517005	-0.059662	4.191454
299.018503	5992.845431	15.522010	-0.059659	4.188771
298.817670	5984.881058	15.527015	-0.059617	4.186092
298.735719	5976.895902	15.532019	-0.059597	4.183407
298.936267	5968.902448	15.537024	-0.059629	4.180719
298.725014	5960.943697	15.542029	-0.059584	4.178037
298.936536	5952.906365	15.547034	-0.059619	4.175332
298.853867	5944.916859	15.552039	-0.059598	4.172637
298.855096	5936.849376	15.557043	-0.059593	4.169916
298.773090	5928.932236	15.562048	-0.059573	4.167243
298.556890	5920.889667	15.567053	-0.059527	4.164524
298.312369	5912.937398	15.572058	-0.059477	4.161833
298.414493	5904.943014	15.577063	-0.059491	4.159130
298.418978	5896.903530	15.582067	-0.059486	4.156410
298.420448	5888.894299	15.587072	-0.059481	4.153697
298.467917	5880.841800	15.592077	-0.059485	4.150969
298.361144	5872.889962	15.597082	-0.059460	4.148271
298.285182	5864.877923	15.602087	-0.059441	4.145552
298.151651	5856.891520	15.607091	-0.059411	4.142838
298.193744	5848.922779	15.612096	-0.059414	4.140131
297.984609	5840.920145	15.617101	-0.059370	4.137408
298.018669	5832.881441	15.622106	-0.059371	4.134673
298.027266	5824.864518	15.627111	-0.059367	4.131944
298.052877	5816.836728	15.632115	-0.059367	4.129209
298.145202	5808.895217	15.637120	-0.059379	4.126503
297.950122	5800.873897	15.642125	-0.059337	4.123765
298.077321	5792.901394	15.647130	-0.059356	4.121045
297.955003	5784.944855	15.652135	-0.059328	4.118326
297.746058	5776.895392	15.657139	-0.059284	4.115572
297.721874	5768.873020	15.662144	-0.059274	4.112827
297.591972	5760.845271	15.667149	-0.059245	4.110078
297.802509	5752.879773	15.672154	-0.059279	4.107353
297.789872	5744.866666	15.677159	-0.059272	4.104606
297.547750	5736.887428	15.682163	-0.059221	4.101867
297.302019	5728.906488	15.687168	-0.059171	4.099125
297.296172	5720.892056	15.692173	-0.059164	4.096372
297.446950	5712.911656	15.697178	-0.059187	4.093632
297.444018	5704.865197	15.702183	-0.059182	4.090865
297.450723	5696.880057	15.707187	-0.059178	4.088117
297.219084	5688.892149	15.712192	-0.059129	4.085363
297.043659	5680.936561	15.717197	-0.059092	4.082620
297.163811	5672.918909	15.722202	-0.059109	4.079857
297.035697	5664.964186	15.727207	-0.059080	4.077110
297.135021	5656.909327	15.732211	-0.059093	4.074331
297.022231	5648.925124	15.737216	-0.059067	4.071570
297.027361	5640.895723	15.742221	-0.059063	4.068794
297.081403	5632.911372	15.747226	-0.059068	4.066033
296.823561	5624.954713	15.752231	-0.059015	4.063274
296.834085	5616.926218	15.757235	-0.059012	4.060493
296.842565	5608.995128	15.762240	-0.059008	4.057743
296.663871	5600.933017	15.767245	-0.058970	4.054944
296.811326	5592.899325	15.772250	-0.058992	4.052157
296.568766	5584.910310	15.777255	-0.058942	4.049378
296.504611	5576.923194	15.782259	-0.058925	4.046600
296.565699	5568.984005	15.787264	-0.058931	4.043839
296.293063	5560.942951	15.792269	-0.058875	4.041036
296.324195	5552.984603	15.797274	-0.058876	4.038264
296.326662	5544.945173	15.802279	-0.058871	4.035461
296.263885	5536.811182	15.807283	-0.058854	4.032623
296.164622	5528.869538	15.812288	-0.058830	4.029849
296.188426	5520.879083	15.817293	-0.058830	4.027058
296.286077	5512.883000	15.822298	-0.058843	4.024264
296.189121	5504.940868	15.827303	-0.058820	4.021484
296.046661	5496.945601	15.832307	-0.058788	4.018683
296.062935	5488.950935	15.837312	-0.058786	4.015883
295.956314	5480.895931	15.842317	-0.058761	4.013057
295.789570	5472.877727	15.847322	-0.058725	4.010242
295.760050	5464.927707	15.852327	-0.058714	4.007450
295.872570	5456.889969	15.857331	-0.058730	4.004628
295.870506	5448.977413	15.862336	-0.058724	4.001847
295.582631	5440.918865	15.867341	-0.058666	3.999007
295.623714	5432.954416	15.872346	-0.058668	3.996204
295.567085	5424.905109	15.877351	-0.058653	3.993367
295.466844	5416.868815	15.882355	-0.058629	3.990533
295.473953	5408.932533	15.887360	-0.058625	3.987733
295.376910	5400.888076	15.892365	-0.058602	3.984891
295.250568	5392.973518	15.897370	-0.058573	3.982093
295.276321	5384.927900	15.902375	-0.058573	3.979249
295.226488	5376.935590	15.907379	-0.058558	3.976420
295.297982	5368.927560	15.912384	-0.058567	3.973586
295.112221	5360.871017	15.917389	-0.058527	3.970729
295.178413	5352.925761	15.922394	-0.058534	3.967912
295.114611	5344.920043	15.927399	-0.058517	3.965071
294.908211	5336.959277	15.932403	-0.058473	3.962241
294.967129	5328.989218	15.937408	-0.058479	3.959410
294.856971	5321.009105	15.942413	-0.058454	3.956570
294.904722	5312.980826	15.947418	-0.058457	3.953714
294.685153	5304.935092	15.952423	-0.058411	3.950845
294.760846	5296.925017	15.957427	-0.058420	3.947992
294.818318	5288.948709	15.962432	-0.058426	3.945149
294.521021	5280.969821	15.967437	-0.058365	3.942296
294.664735	5272.972068	15.972442	-0.058387	3.939442
294.736649	5264.986154	15.977447	-0.058395	3.936589
294.616126	5256.973481	15.982451	-0.058368	3.933722
294.560494	5248.991443	15.987456	-0.058352	3.930864
294.531641	5240.993016	15.992461	-0.058342	3.927998
294.693667	5232.950127	15.997466	-0.058367	3.925118
294.501265	5225.009768	16.002471	-0.058326	3.922267
294.290926	5216.991831	16.007475	-0.058282	3.919385
294.297105	5209.059453	16.012480	-0.058278	3.916535
294.324634	5200.970315	16.017485	-0.058278	3.913628
294.328457	5192.969915	16.022490	-0.058273	3.910750
294.147538	5185.004658	16.027495	-0.058234	3.907879
294.062692	5176.985908	16.032499	-0.058213	3.904988
294.077857	5169.008740	16.037504	-0.058211	3.902112
294.004258	5160.995273	16.042509	-0.058192	3.899219
294.129382	5153.016514	16.047514	-0.058210	3.896340
293.938011	5144.998547	16.052519	-0.058170	3.893439
293.818069	5136.954483	16.057523	-0.058142	3.890528
293.926881	5129.033144	16.062528	-0.058157	3.887663
293.764477	5120.949880	16.067533	-0.058122	3.884733
293.658702	5113.035158	16.072538	-0.058097	3.881862
293.778610	5105.019884	16.077543	-0.058114	3.878957
293.645710	5097.017835	16.082547	-0.058084	3.876050
293.674184	5088.815751	16.087552	-0.058084	3.873071
293.696188	5080.755947	16.092557	-0.058083	3.870141
293.536049	5072.901492	16.097562	-0.058049	3.867280
293.364030	5064.923271	16.102567	-0.058011	3.864372
293.290681	5056.995531	16.107571	-0.057993	3.861482
293.215113	5049.013118	16.112576	-0.057973	3.858570
293.296519	5040.972720	16.117581	-0.057983	3.855637
293.329345	5032.971802	16.122586	-0.057984	3.852716
293.198621	5024.991804	16.127591	-0.057955	3.849797
293.036742	5017.005967	16.132595	-0.057920	3.846873
292.922595	5009.020257	16.137600	-0.057893	3.843948
292.869267	5001.016046	16.142605	-0.057878	3.841015
292.969565	4993.057189	16.147610	-0.057892	3.838099
292.776746	4985.063551	16.152615	-0.057851	3.835162
292.721255	4976.996260	16.157619	-0.057835	3.832199
293.033348	4968.982722	16.162624	-0.057888	3.829261
292.820378	4960.997748	16.167629	-0.057844	3.826321
292.698795	4953.033394	16.172634	-0.057816	3.823387
292.547241	4945.054017	16.177639	-0.057782	3.820445
292.702282	4937.053392	16.182643	-0.057806	3.817500
292.706289	4929.053053	16.187648	-0.057802	3.814549
292.574060	4921.053971	16.192653	-0.057772	3.811593
292.493065	4913.080200	16.197658	-0.057752	3.808646
292.441481	4905.086481	16.202663	-0.057737	3.805689
292.474133	4897.083201	16.207667	-0.057738	3.802729
292.413119	4889.104185	16.212672	-0.057722	3.799773
292.369049	4881.127062	16.217677	-0.057708	3.796815
292.327571	4873.097969	16.222682	-0.057695	3.793837
292.180492	4865.052766	16.227687	-0.057663	3.790847
292.132590	4857.055235	16.232691	-0.057649	3.787876
292.181253	4849.050794	16.237696	-0.057653	3.784901
292.109792	4841.115054	16.242701	-0.057634	3.781947
292.261832	4833.088554	16.247706	-0.057657	3.778962
292.059421	4825.111088	16.252711	-0.057615	3.775985
291.881515	4817.078302	16.257715	-0.057576	3.772985
291.986298	4809.095351	16.262720	-0.057591	3.770008
292.020833	4801.100307	16.267725	-0.057592	3.767022
291.856986	4793.107626	16.272730	-0.057556	3.764031
291.744142	4785.116641	16.277735	-0.057530	3.761039
291.714068	4777.100404	16.282739	-0.057520	3.758036
291.792577	4769.123993	16.287744	-0.057529	3.755049
291.820384	4761.082918	16.292749	-0.057529	3.752034
291.774834	4753.101829	16.297754	-0.057516	3.749038
291.709021	4745.071890	16.302759	-0.057498	3.746020
291.526319	4737.114566	16.307763	-0.057459	3.743025
291.700273	4729.114383	16.312768	-0.057486	3.740019
291.582471	4721.140226	16.317773	-0.057459	3.737013
291.478266	4713.150996	16.322778	-0.057435	3.734000
291.438450	4705.126203	16.327783	-0.057422	3.730973
291.372532	4697.140993	16.332787	-0.057405	3.727958
291.242441	4689.115069	16.337792	-0.057375	3.724923
291.132211	4681.185305	16.342797	-0.057350	3.721922
291.133272	4673.180761	16.347802	-0.057345	3.718893
290.981054	4665.196533	16.352807	-0.057311	3.715866
290.952348	4657.133666	16.357811	-0.057301	3.712810
291.036722	4649.136100	16.362816	-0.057311	3.709778
291.007823	4641.128412	16.367821	-0.057301	3.706738
290.829805	4633.142587	16.372826	-0.057263	3.703700
290.731763	4625.166483	16.377831	-0.057239	3.700664
290.882737	4617.189993	16.382835	-0.057262	3.697633
290.903741	4609.198863	16.387840	-0.057261	3.694590
290.660588	4601.192092	16.392845	-0.057211	3.691532
290.683052	4593.232926	16.397850	-0.057210	3.688496
290.789795	4585.184103	16.402855	-0.057224	3.685425
290.525369	4577.237208	16.407859	-0.057170	3.682382
290.515339	4569.242826	16.412864	-0.057163	3.679324
290.302300	4561.262715	16.417869	-0.057118	3.676264
290.314986	4553.237835	16.422874	-0.057115	3.673190
290.294693	4545.196617	16.427879	-0.057107	3.670107
290.271857	4537.200564	16.432883	-0.057097	3.667038
290.247154	4529.229222	16.437888	-0.057087	3.663976
290.148504	4521.232138	16.442893	-0.057064	3.660899
290.297951	4513.257703	16.447898	-0.057087	3.657835
290.226973	4505.243866	16.452903	-0.057068	3.654748
290.030183	4497.239622	16.457907	-0.057027	3.651659
290.076784	4489.240411	16.462912	-0.057030	3.648575
290.011711	4481.201328	16.467917	-0.057013	3.645470
289.922741	4473.290298	16.472922	-0.056991	3.642411
289.905157	4465.253587	16.477927	-0.056983	3.639303
289.708199	4457.297267	16.482931	-0.056941	3.636219
289.824780	4449.282047	16.487936	-0.056958	3.633118
289.683061	4441.239809	16.492941	-0.056926	3.629996
289.553565	4433.268064	16.497946	-0.056897	3.626900
289.629418	4425.249655	16.502951	-0.056906	3.623788
289.657791	4417.263871	16.507955	-0.056906	3.620685
289.680649	4409.334245	16.512960	-0.056905	3.617601
289.686860	4401.280276	16.517965	-0.056901	3.614466
289.563386	4393.279980	16.522970	-0.056873	3.611345
289.234605	4385.329021	16.527975	-0.056807	3.608235
289.215661	4377.284201	16.532979	-0.056798	3.605095
289.284012	4369.365675	16.537984	-0.056806	3.602003
289.052703	4361.358528	16.542989	-0.056757	3.598865
289.333367	4353.357365	16.547994	-0.056805	3.595742
289.248040	4345.356314	16.552999	-0.056783	3.592606
289.009448	4337.334186	16.558003	-0.056734	3.589454
288.984231	4329.374788	16.563008	-0.056724	3.586330
289.039076	4321.370533	16.568013	-0.056729	3.583188
288.989615	4313.376786	16.573018	-0.056715	3.580045
289.005253	4305.413964	16.578023	-0.056713	3.576912
288.935868	4297.401636	16.583027	-0.056695	3.573755
288.989039	4289.404197	16.588032	-0.056699	3.570605
288.800749	4281.411514	16.593037	-0.056659	3.567447
288.794422	4273.414362	16.598042	-0.056653	3.564289
288.851947	4265.437817	16.603047	-0.056658	3.561139
288.560534	4257.447244	16.608051	-0.056599	3.557970
288.360310	4249.465921	16.613056	-0.056557	3.554804
288.444823	4241.338585	16.618061	-0.056567	3.551587
288.619592	4233.352784	16.623066	-0.056595	3.548425
288.665425	4225.370967	16.628071	-0.056598	3.545258
288.515721	4217.402098	16.633075	-0.056565	3.542087
288.511180	4209.418679	16.638080	-0.056559	3.538912
288.224867	4201.445362	16.643085	-0.056501	3.535730
288.112058	4193.436650	16.648090	-0.056475	3.532537
288.376758	4185.400742	16.653095	-0.056519	3.529340
288.107462	4177.430806	16.658099	-0.056463	3.526152
288.010891	4169.520844	16.663104	-0.056440	3.522989
288.048796	4161.461164	16.668109	-0.056442	3.519768
288.004543	4153.491478	16.673114	-0.056429	3.516577
288.056892	4145.459406	16.678119	-0.056433	3.513361
287.903270	4137.449536	16.683123	-0.056400	3.510145
288.027814	4129.479555	16.688128	-0.056418	3.506951
287.760042	4121.500900	16.693133	-0.056363	3.503738
287.706307	4113.515636	16.698138	-0.056348	3.500526
287.798395	4105.544377	16.703143	-0.056360	3.497321
287.883043	4097.528274	16.708147	-0.056370	3.494095
287.720734	4089.545554	16.713152	-0.056335	3.490872
287.686187	4081.549582	16.718157	-0.056323	3.487645
287.468712	4073.594528	16.723162	-0.056278	3.484425
287.224356	4065.639759	16.728167	-0.056227	3.481202
287.181231	4057.632068	16.733171	-0.056214	3.477960
287.182304	4049.609154	16.738176	-0.056209	3.474711
287.210332	4041.534678	16.743181	-0.056209	3.471438
286.977331	4033.584425	16.748186	-0.056161	3.468205
287.029478	4025.580077	16.753191	-0.056165	3.464955
286.915860	4017.615485	16.758195	-0.056139	3.461714
286.925476	4009.644064	16.763200	-0.056136	3.458470
286.917352	4001.606446	16.768205	-0.056129	3.455196
287.064230	3993.625370	16.773210	-0.056151	3.451947
286.903953	3985.608157	16.778215	-0.056116	3.448670
286.730153	3977.615004	16.783219	-0.056079	3.445400
286.883530	3969.678130	16.788224	-0.056102	3.442160
286.749805	3961.657326	16.793229	-0.056072	3.438873
286.583488	3953.674304	16.798234	-0.056036	3.435597
286.636550	3945.663021	16.803239	-0.056041	3.432314
286.591889	3937.630029	16.808243	-0.056027	3.429016
286.716417	3929.657164	16.813248	-0.056045	3.425745
286.552798	3921.681878	16.818253	-0.056010	3.422460
286.637705	3913.703950	16.823258	-0.056021	3.419179
286.405585	3905.733768	16.828263	-0.055972	3.415887
286.219559	3897.730535	16.833267	-0.055932	3.412580
286.308059	3889.714149	16.838272	-0.055944	3.409274
286.159335	3881.719717	16.843277	-0.055911	3.405966
285.844220	3873.786824	16.848282	-0.055847	3.402674
285.904894	3865.771178	16.853287	-0.055853	3.399357
286.089278	3857.770408	16.858291	-0.055883	3.396048
286.135284	3849.724145	16.863296	-0.055886	3.392712
286.156902	3841.677286	16.868301	-0.055885	3.389371
286.136105	3833.712463	16.873306	-0.055876	3.386060
285.926289	3825.807243	16.878311	-0.055832	3.382764
285.903155	3817.784048	16.883315	-0.055822	3.379422
285.842412	3809.825109	16.888320	-0.055806	3.376102
285.772442	3801.814985	16.893325	-0.055788	3.372757
285.606235	3793.823202	16.898330	-0.055752	3.369413
285.607781	3785.829733	16.903335	-0.055747	3.366071
285.526925	3777.845969	16.908339	-0.055727	3.362727
285.576022	3769.867347	16.913344	-0.055731	3.359386
285.387914	3761.882607	16.918349	-0.055691	3.356030
285.430891	3753.840885	16.923354	-0.055693	3.352656
285.231167	3745.851761	16.928359	-0.055651	3.349292
285.231524	3737.838778	16.933363	-0.055646	3.345921
285.306988	3729.901530	16.938368	-0.055655	3.342582
285.256274	3721.876436	16.943373	-0.055640	3.339198
285.025304	3713.951980	16.948378	-0.055592	3.335846
285.148412	3705.920748	16.953383	-0.055610	3.332459
285.184865	3697.886688	16.958387	-0.055612	3.329064
285.055363	3689.932004	16.963392	-0.055582	3.325692
284.941064	3681.959820	16.968397	-0.055556	3.322311
284.875152	3673.980551	16.973402	-0.055539	3.318925
284.838798	3665.992174	16.978407	-0.055527	3.315532
284.655642	3657.977132	16.983411	-0.055488	3.312120
284.709591	3649.981889	16.988416	-0.055492	3.308721
284.453994	3641.997913	16.993421	-0.055440	3.305312
284.444689	3634.028384	16.998426	-0.055433	3.301914
284.601522	3626.024583	17.003431	-0.055457	3.298505
284.434412	3618.021172	17.008435	-0.055421	3.295080
284.501086	3610.050645	17.013440	-0.055428	3.291675
284.436022	3602.016230	17.018445	-0.055411	3.288233
284.276900	3594.035794	17.023450	-0.055376	3.284808
284.238934	3586.111129	17.028455	-0.055364	3.281407
284.071522	3578.119093	17.033459	-0.055328	3.277969
284.307871	3570.092005	17.038464	-0.055366	3.274528
284.206969	3562.079666	17.043469	-0.055342	3.271077
283.981557	3554.116769	17.048474	-0.055295	3.267638
284.015374	3546.139658	17.053479	-0.055297	3.264200
284.110431	3538.121295	17.058483	-0.055309	3.260743
284.057870	3530.167400	17.063488	-0.055294	3.257304
283.918097	3522.145468	17.068493	-0.055263	3.253829
283.944119	3514.135077	17.073498	-0.055263	3.250361
283.783175	3506.181261	17.078503	-0.055228	3.246907
283.596768	3498.197336	17.083507	-0.055188	3.243435
283.671368	3490.222527	17.088512	-0.055197	3.239973
283.760682	3482.235482	17.093517	-0.055208	3.236504
283.587761	3474.185798	17.098522	-0.055171	3.232992
283.480492	3466.181128	17.103527	-0.055146	3.229499
283.511863	3458.169483	17.108531	-0.055146	3.226005
283.675186	3450.212853	17.113536	-0.055172	3.222537
283.423522	3442.242616	17.118541	-0.055120	3.219042
283.195647	3434.287501	17.123546	-0.055072	3.215550
283.248746	3426.287863	17.128551	-0.055077	3.212047
283.187776	3418.274164	17.133555	-0.055060	3.208529
283.327347	3410.269680	17.138560	-0.055081	3.205020
283.380636	3402.313230	17.143565	-0.055086	3.201524
283.189025	3394.348787	17.148570	-0.055045	3.198011
283.000285	3386.372386	17.153575	-0.055005	3.194489
283.195462	3378.326868	17.158579	-0.055036	3.190948
283.058103	3370.356295	17.163584	-0.055006	3.187423
282.747663	3362.375035	17.168589	-0.054943	3.183881
282.733782	3354.410575	17.173594	-0.054935	3.180356
282.921657	3346.415312	17.178599	-0.054965	3.176822
282.667601	3338.417580	17.183603	-0.054912	3.173263
282.662481	3330.419892	17.188608	-0.054906	3.169712
282.560204	3322.418727	17.193613	-0.054882	3.166151
282.630815	3314.453482	17.198618	-0.054890	3.162609
282.352729	3306.487266	17.203623	-0.054833	3.159047
282.322396	3298.477604	17.208627	-0.054822	3.155473
282.395642	3290.470519	17.213632	-0.054831	3.151901
282.422169	3282.458158	17.218637	-0.054831	3.148320
282.205429	3274.487567	17.223642	-0.054785	3.144743
282.378626	3266.516798	17.228647	-0.054812	3.141179
282.215556	3258.541842	17.233651	-0.054777	3.137594
282.340076	3250.541066	17.238656	-0.054795	3.134006
282.029662	3242.560007	17.243661	-0.054732	3.130404
281.913439	3234.576195	17.248666	-0.054705	3.126805
281.881825	3226.610638	17.253671	-0.054694	3.123214
281.887527	3218.597341	17.258675	-0.054690	3.119599
281.978680	3210.653984	17.263680	-0.054702	3.116015
281.730201	3202.627008	17.268685	-0.054651	3.112373
281.832748	3194.609271	17.273690	-0.054665	3.108748
281.869026	3186.632878	17.278695	-0.054666	3.105134
281.690249	3178.684373	17.283699	-0.054628	3.101519
281.780833	3170.701244	17.288704	-0.054640	3.097895
281.684623	3162.688427	17.293709	-0.054617	3.094246
281.744873	3154.674273	17.298714	-0.054623	3.090599
281.520130	3146.767202	17.303719	-0.054576	3.086983
281.466467	3138.731369	17.308723	-0.054561	3.083313
281.524843	3130.788764	17.313728	-0.054566	3.079685
281.441177	3122.814565	17.318733	-0.054546	3.076032
281.469647	3114.733685	17.323738	-0.054546	3.072332
281.385594	3106.742609	17.328743	-0.054525	3.068662
281.248297	3098.754301	17.333747	-0.054494	3.064987
281.345359	3090.806826	17.338752	-0.054507	3.061338
281.204952	3082.816339	17.343757	-0.054476	3.057653
281.082147	3074.856782	17.348762	-0.054448	3.053979
281.127163	3066.853901	17.353767	-0.054451	3.050288
280.876489	3058.892955	17.358771	-0.054400	3.046598
280.958466	3050.913766	17.363776	-0.054410	3.042911
280.923448	3042.932641	17.368781	-0.054398	3.039213
280.937534	3034.949470	17.373786	-0.054396	3.035512
280.821793	3026.955136	17.378791	-0.054369	3.031795
280.930525	3018.936751	17.383795	-0.054384	3.028073
280.859919	3010.958789	17.388800	-0.054366	3.024356
280.636618	3003.013862	17.393805	-0.054319	3.020643
280.640852	2995.038477	17.398810	-0.054315	3.016922
280.563964	2987.036619	17.403815	-0.054295	3.013181
280.570423	2979.024049	17.408819	-0.054291	3.009433
280.540731	2971.055878	17.413824	-0.054281	3.005700
280.507159	2963.096034	17.418829	-0.054269	3.001966
280.429996	2955.120109	17.423834	-0.054250	2.998218
280.454362	2947.126283	17.428839	-0.054249	2.994462
280.297181	2939.107878	17.433843	-0.054215	2.990680
280.228290	2931.134090	17.438848	-0.054197	2.986919
280.244981	2923.124979	17.443853	-0.054195	2.983141
280.163988	2915.180587	17.448858	-0.054175	2.979383
280.207477	2907.217238	17.453863	-0.054178	2.975619
279.975346	2899.220091	17.458867	-0.054129	2.971819
280.144687	2891.220854	17.463872	-0.054156	2.968034
280.109436	2883.239080	17.468877	-0.054144	2.964242
279.836455	2875.304074	17.473882	-0.054088	2.960455
279.794125	2867.331103	17.478887	-0.054075	2.956657
279.825564	2859.285229	17.483891	-0.054076	2.952824
279.539820	2851.313903	17.488896	-0.054018	2.949004
279.368477	2843.329657	17.493901	-0.053981	2.945179
279.333186	2835.389461	17.498906	-0.053969	2.941378
279.428910	2827.397229	17.503911	-0.053982	2.937553
279.490423	2819.359232	17.508915	-0.053988	2.933699
279.396223	2811.400581	17.513920	-0.053965	2.929871
279.256833	2803.433940	17.518925	-0.053934	2.926031
279.324692	2795.439110	17.523930	-0.053942	2.922184
279.205667	2787.507467	17.528935	-0.053914	2.918352
279.162452	2779.503101	17.533939	-0.053901	2.914483
279.102050	2771.424173	17.538944	-0.053885	2.910573
278.937217	2763.451321	17.543949	-0.053849	2.906703
278.874625	2755.496620	17.548954	-0.053832	2.902843
279.222607	2747.513850	17.553959	-0.053892	2.898985
278.973840	2739.546884	17.558963	-0.053840	2.895098
278.982611	2731.570044	17.563968	-0.053837	2.891215
278.826568	2723.585644	17.568973	-0.053803	2.887314
278.833582	2715.631782	17.573978	-0.053799	2.883432
278.641153	2707.691590	17.578983	-0.053758	2.879540
278.633773	2699.703448	17.583987	-0.053752	2.875629
278.477765	2691.694336	17.588992	-0.053717	2.871695
278.352829	2683.699814	17.593997	-0.053689	2.867764
278.558584	2675.693372	17.599002	-0.053722	2.863840
278.594029	2667.745360	17.604007	-0.053724	2.859930
278.328965	2659.793751	17.609011	-0.053669	2.855996
278.315733	2651.800964	17.614016	-0.053662	2.852051
278.249987	2643.804316	17.619021	-0.053644	2.848095
278.140771	2635.839467	17.624026	-0.053619	2.844147
278.080290	2627.895348	17.629031	-0.053602	2.840206
278.104546	2619.903053	17.634035	-0.053602	2.836241
277.992773	2611.920368	17.639040	-0.053576	2.832267
278.057730	2603.886285	17.644045	-0.053583	2.828272
277.950028	2595.915675	17.649050	-0.053558	2.824293
278.035161	2587.955671	17.654055	-0.053568	2.820325
277.654566	2580.018074	17.659059	-0.053493	2.816336
277.877087	2572.011865	17.664064	-0.053529	2.812342
277.865074	2564.007627	17.669069	-0.053521	2.808329
277.533072	2556.063917	17.674074	-0.053455	2.804323
277.646419	2548.096781	17.679079	-0.053471	2.800324
277.527408	2540.123664	17.684083	-0.053443	2.796304
277.357731	2532.142539	17.689088	-0.053407	2.792270
277.483636	2524.112998	17.694093	-0.053425	2.788224
277.514679	2516.120193	17.699098	-0.053425	2.784185
277.627348	2508.159716	17.704103	-0.053441	2.780161
277.228981	2500.239782	17.709107	-0.053362	2.776122
277.301070	2492.233972	17.714112	-0.053370	2.772060
277.139464	2484.259668	17.719117	-0.053335	2.767996
276.886504	2476.323123	17.724122	-0.053283	2.763939
276.877449	2468.357066	17.729127	-0.053276	2.759875
276.889409	2460.367310	17.734131	-0.053273	2.755795
276.842616	2452.299903	17.739136	-0.053259	2.751665
276.795185	2444.309862	17.744141	-0.053245	2.747568
276.734369	2436.349141	17.749146	-0.053229	2.743480
276.719188	2428.396772	17.754151	-0.053221	2.739393
276.620845	2420.424251	17.759155	-0.053198	2.735284
276.541533	2412.456070	17.764160	-0.053178	2.731172
276.498526	2404.482343	17.769165	-0.053165	2.727054
276.526604	2396.498385	17.774170	-0.053165	2.722928
276.492155	2388.556824	17.779175	-0.053153	2.718814
276.507251	2380.561853	17.784179	-0.053151	2.714669
276.450483	2372.582229	17.789184	-0.053135	2.710522
276.193915	2364.621273	17.794189	-0.053082	2.706365
276.328925	2356.632523	17.799194	-0.053102	2.702212
276.556287	2348.665260	17.804199	-0.053140	2.698069
276.215263	2340.709533	17.809203	-0.053071	2.693891
276.092825	2332.719850	17.814208	-0.053043	2.689702
276.212886	2324.743295	17.819213	-0.053060	2.685528
276.153437	2316.803647	17.824218	-0.053044	2.681356
276.022213	2308.854191	17.829223	-0.053015	2.677168
275.848535	2300.841222	17.834227	-0.052977	2.672937
275.910734	2292.839120	17.839232	-0.052984	2.668720
275.776496	2284.867521	17.844237	-0.052954	2.664500
275.785648	2276.901837	17.849242	-0.052950	2.660286
275.569180	2268.973248	17.854247	-0.052905	2.656070
275.375420	2260.986436	17.859251	-0.052864	2.651818
275.462366	2253.002373	17.864256	-0.052875	2.647578
275.262205	2245.033304	17.869261	-0.052832	2.643322
275.324178	2237.065882	17.874266	-0.052839	2.639076
275.417129	2229.110075	17.879271	-0.052851	2.634831
275.380145	2221.076878	17.884275	-0.052839	2.630530
275.368881	2213.135737	17.889280	-0.052832	2.626273
275.122935	2205.193657	17.894285	-0.052781	2.621993
275.008318	2197.222391	17.899290	-0.052754	2.617699
275.068780	2189.245255	17.904295	-0.052760	2.613406
275.006954	2181.243697	17.909299	-0.052744	2.609085
274.932549	2173.295948	17.914304	-0.052725	2.604785
274.860028	2165.348451	17.919309	-0.052706	2.600478
274.867891	2157.384035	17.924314	-0.052703	2.596160
274.770227	2149.277426	17.929319	-0.052679	2.591750
274.529771	2141.271557	17.934323	-0.052629	2.587379
274.689513	2133.327559	17.939328	-0.052654	2.583060
274.511345	2125.406999	17.944333	-0.052616	2.578724
274.511962	2117.446951	17.949338	-0.052611	2.574372
274.692354	2109.456454	17.954343	-0.052639	2.570008
274.501046	2101.502518	17.959347	-0.052598	2.565630
274.556080	2093.564190	17.964352	-0.052604	2.561271
274.316071	2085.647338	17.969357	-0.052554	2.556896
274.418899	2077.639256	17.974362	-0.052568	2.552487
274.190410	2069.694727	17.979367	-0.052520	2.548082
274.023405	2061.721058	17.984371	-0.052484	2.543658
274.204518	2053.741413	17.989376	-0.052513	2.539247
274.034636	2045.781615	17.994381	-0.052476	2.534814
273.952438	2037.814592	17.999386	-0.052455	2.530377
274.101002	2029.830798	18.004391	-0.052478	2.525938
273.912964	2021.900808	18.009395	-0.052438	2.521497
273.912122	2013.953449	18.014400	-0.052433	2.517053
273.795174	2005.967055	18.019405	-0.052406	2.512570
273.618735	1997.979262	18.024410	-0.052368	2.508074
273.747785	1990.001913	18.029415	-0.052387	2.503598
273.560764	1982.073281	18.034419	-0.052347	2.499119
273.486205	1974.117133	18.039424	-0.052328	2.494624
273.264481	1966.148266	18.044429	-0.052281	2.490103
273.389477	1958.146479	18.049434	-0.052300	2.485580
273.290399	1950.219210	18.054439	-0.052276	2.481075
273.103815	1942.285623	18.059443	-0.052236	2.476552
273.311251	1934.278012	18.064448	-0.052270	2.472008
273.323383	1926.284116	18.069453	-0.052267	2.467448
273.006129	1918.378119	18.074458	-0.052203	2.462906
272.986781	1910.426298	18.079463	-0.052194	2.458351
273.028751	1902.425215	18.084467	-0.052197	2.453764
273.068075	1894.446730	18.089472	-0.052199	2.449182
272.839879	1886.523303	18.094477	-0.052151	2.444602
272.654960	1878.592968	18.099482	-0.052112	2.440013
272.717980	1870.633245	18.104487	-0.052118	2.435417
272.659904	1862.571114	18.109491	-0.052102	2.430744
272.582653	1854.635360	18.114496	-0.052083	2.426134
272.216445	1846.711513	18.119501	-0.052010	2.421500
272.221405	1838.745754	18.124506	-0.052005	2.416860
272.307886	1830.767127	18.129511	-0.052016	2.412211
272.031892	1822.809677	18.134515	-0.051960	2.407537
272.149661	1814.859286	18.139520	-0.051977	2.402889
272.066678	1806.899579	18.144525	-0.051956	2.398210
272.158779	1798.924472	18.149530	-0.051968	2.393527
272.222051	1790.945455	18.154535	-0.051975	2.388831
272.055947	1782.998679	18.159539	-0.051939	2.384126
271.960936	1775.077434	18.164544	-0.051916	2.379432
272.029424	1767.112378	18.169549	-0.051924	2.374716
271.856844	1759.152327	18.174554	-0.051887	2.369974
271.702357	1751.210075	18.179559	-0.051853	2.365235
271.375676	1743.295462	18.184563	-0.051787	2.360489
271.465720	1735.332024	18.189568	-0.051798	2.355738
271.442690	1727.324291	18.194573	-0.051789	2.350942
271.338696	1719.364364	18.199578	-0.051765	2.346158
271.458050	1711.402479	18.204583	-0.051782	2.341381
271.398893	1703.454508	18.209587	-0.051766	2.336588
271.365079	1695.488700	18.214592	-0.051754	2.331776
271.209039	1687.548715	18.219597	-0.051720	2.326960
271.282158	1679.585368	18.224602	-0.051728	2.322139
271.360178	1671.659138	18.229607	-0.051738	2.317331
271.220229	1663.687550	18.234611	-0.051707	2.312467
270.964477	1655.755014	18.239616	-0.051654	2.307607
270.949895	1647.788782	18.244621	-0.051646	2.302736
270.927938	1639.840922	18.249626	-0.051637	2.297866
270.926234	1631.885294	18.254631	-0.051632	2.292982
270.713954	1623.943066	18.259635	-0.051587	2.288078
270.766215	1615.996049	18.264640	-0.051592	2.283183
270.835595	1608.038179	18.269645	-0.051599	2.278272
270.755431	1600.066395	18.274650	-0.051579	2.273330
270.778568	1592.057021	18.279655	-0.051579	2.268362
270.579397	1584.134009	18.284659	-0.051536	2.263417
270.486635	1576.221458	18.289664	-0.051514	2.258478
270.326548	1568.277186	18.294669	-0.051479	2.253502
270.479689	1560.287895	18.299674	-0.051503	2.248514
270.135781	1552.392766	18.304679	-0.051433	2.243530
270.074334	1544.447565	18.309683	-0.051417	2.238529
270.066775	1536.495812	18.314688	-0.051410	2.233517
269.996413	1528.522774	18.319693	-0.051392	2.228475
269.881177	1520.579015	18.324698	-0.051366	2.223436
270.104821	1512.626288	18.329703	-0.051402	2.218410
269.784292	1504.705663	18.334707	-0.051337	2.213344
269.807705	1496.751922	18.339712	-0.051337	2.208277
269.728392	1488.806684	18.344717	-0.051317	2.203193
269.811719	1480.853520	18.349722	-0.051327	2.198108
269.680305	1472.928549	18.354727	-0.051298	2.193010
269.489576	1464.958963	18.359731	-0.051257	2.187865
269.563456	1457.010251	18.364736	-0.051266	2.182746
269.335642	1449.112444	18.369741	-0.051218	2.177621
269.208823	1441.154573	18.374746	-0.051189	2.172453
269.462770	1433.181596	18.379751	-0.051232	2.167299
269.018010	1425.275671	18.384755	-0.051144	2.162111
269.018978	1417.357372	18.389760	-0.051139	2.156944
269.025313	1409.395530	18.394765	-0.051135	2.151736
269.208081	1401.399707	18.399770	-0.051164	2.146510
269.115656	1393.502848	18.404775	-0.051142	2.141311
268.854291	1385.587400	18.409779	-0.051088	2.136071
268.929571	1377.627972	18.414784	-0.051097	2.130820
268.931658	1369.674574	18.419789	-0.051092	2.125554
268.618913	1361.790559	18.424794	-0.051029	2.120290
268.885054	1353.829232	18.429799	-0.051073	2.115018
268.508579	1345.844807	18.434803	-0.050998	2.109655
268.398463	1337.927604	18.439808	-0.050972	2.104349
268.445247	1329.995910	18.444813	-0.050976	2.099035
268.516501	1322.041514	18.449818	-0.050984	2.093695
268.419737	1314.112009	18.454823	-0.050961	2.088341
268.411101	1306.160808	18.459827	-0.050954	2.082967
268.434180	1298.257721	18.464832	-0.050954	2.077616
268.216924	1290.344947	18.469837	-0.050908	2.072220
268.005761	1282.420217	18.474842	-0.050864	2.066803
268.288738	1274.454180	18.479847	-0.050911	2.061392
267.941080	1266.559892	18.484851	-0.050841	2.055953
267.778127	1258.641342	18.489856	-0.050806	2.050502
267.673624	1250.699833	18.494861	-0.050782	2.045026
267.605475	1242.790816	18.499866	-0.050764	2.039561
267.645696	1234.863013	18.504871	-0.050766	2.034080
267.517384	1226.897481	18.509875	-0.050737	2.028540
267.513915	1218.974402	18.514880	-0.050731	2.023028
267.529802	1211.037864	18.519885	-0.050729	2.017493
267.364610	1203.122819	18.524890	-0.050693	2.011939
267.357559	1195.197927	18.529895	-0.050687	2.006380
267.424146	1187.251954	18.534899	-0.050694	2.000797
267.346773	1179.365974	18.539904	-0.050675	1.995227
267.246901	1171.426275	18.544909	-0.050651	1.989600
267.145270	1163.502539	18.549914	-0.050627	1.983969
267.150877	1155.598775	18.554919	-0.050623	1.978347
266.878438	1147.696134	18.559923	-0.050567	1.972680
266.956672	1139.746033	18.564928	-0.050577	1.967000
266.985995	1131.825451	18.569933	-0.050577	1.961320
266.781353	1123.946269	18.574938	-0.050534	1.955628
266.873043	1115.954245	18.579943	-0.050546	1.949870
266.792904	1108.027621	18.584947	-0.050526	1.944123
266.737408	1100.133868	18.589952	-0.050511	1.938386
266.439994	1092.240980	18.594957	-0.050450	1.932606
266.655635	1084.284284	18.599962	-0.050485	1.926819
266.715628	1076.373449	18.604967	-0.050491	1.921030
266.328720	1068.510715	18.609971	-0.050414	1.915210
266.586893	1060.543041	18.614976	-0.050457	1.909366
266.441434	1052.648730	18.619981	-0.050425	1.903514
266.076228	1044.782840	18.624986	-0.050352	1.897640
266.087718	1036.859967	18.629991	-0.050349	1.891748
265.975532	1028.935390	18.634995	-0.050323	1.885822
265.819459	1021.064523	18.640000	-0.050289	1.879912
265.771966	1013.159849	18.645005	-0.050275	1.873971
265.719768	1005.221795	18.650010	-0.050260	1.867985
265.801670	997.301727	18.655015	-0.050270	1.862009
265.587789	989.419882	18.660019	-0.050226	1.856009
265.549851	981.502346	18.665024	-0.050213	1.849982
265.536690	973.593945	18.670029	-0.050206	1.843946
265.171324	965.751574	18.675034	-0.050133	1.837898
265.321287	957.817031	18.680039	-0.050156	1.831821
265.117518	949.913073	18.685043	-0.050113	1.825705
265.009997	942.040275	18.690048	-0.050088	1.819604
265.034608	934.133808	18.695053	-0.050087	1.813473
264.793276	926.235601	18.700058	-0.050037	1.807294
264.914041	918.334773	18.705063	-0.050055	1.801137
264.814054	910.450226	18.710067	-0.050031	1.794944
264.922804	902.479192	18.715072	-0.050046	1.788687
265.002616	894.572369	18.720077	-0.050056	1.782455
264.729150	886.730810	18.725082	-0.050000	1.776210
264.546836	878.857196	18.730087	-0.049961	1.769928
264.365099	870.983442	18.735091	-0.049922	1.763624
264.474172	863.092064	18.740096	-0.049937	1.757320
264.371059	855.195057	18.745101	-0.049913	1.750961
264.225893	847.314225	18.750106	-0.049881	1.744587
264.347135	839.434283	18.755111	-0.049898	1.738225
264.039143	831.569498	18.760115	-0.049836	1.731796
264.170746	823.663518	18.765120	-0.049855	1.725366
264.083295	815.812650	18.770125	-0.049834	1.718929
264.090427	807.914720	18.775130	-0.049830	1.712442
263.991375	800.040130	18.780135	-0.049807	1.705935
263.887088	792.171609	18.785139	-0.049782	1.699407
263.921708	784.294580	18.790144	-0.049784	1.692866
263.754838	776.424640	18.795149	-0.049748	1.686278
263.663172	768.572925	18.800154	-0.049726	1.679690
263.605416	760.718702	18.805159	-0.049710	1.673078
263.368683	752.846571	18.810163	-0.049661	1.666401
263.280260	744.996418	18.815168	-0.049639	1.659735
263.407474	737.101826	18.820173	-0.049658	1.653034
263.271589	729.234053	18.825178	-0.049627	1.646293
263.254099	721.394793	18.830183	-0.049619	1.639565
263.176116	713.518476	18.835187	-0.049600	1.632769
263.254823	705.598092	18.840192	-0.049609	1.625927
262.864513	697.808996	18.845197	-0.049531	1.619106
262.844632	689.941646	18.850202	-0.049523	1.612240
262.877807	682.080774	18.855207	-0.049524	1.605357
262.820453	674.238824	18.860211	-0.049508	1.598448
262.740567	666.397375	18.865216	-0.049488	1.591507
262.625885	658.542225	18.870221	-0.049462	1.584518
262.478286	650.727781	18.875226	-0.049429	1.577529
262.347624	642.887232	18.880231	-0.049400	1.570489
262.161007	635.060467	18.885235	-0.049360	1.563420
262.263274	627.212551	18.890240	-0.049374	1.556343
262.299073	619.342780	18.895245	-0.049376	1.549204
262.148253	611.513089	18.900250	-0.049343	1.542041
262.190355	603.683993	18.905255	-0.049346	1.534874
261.876661	595.883964	18.910259	-0.049282	1.527646
261.860980	588.059552	18.915264	-0.049274	1.520407
261.731721	580.252111	18.920269	-0.049245	1.513131
261.665813	572.406596	18.925274	-0.049228	1.505794
261.662348	564.594925	18.930279	-0.049222	1.498463
261.579952	556.766751	18.935283	-0.049202	1.491068
261.696389	548.934886	18.940288	-0.049219	1.483663
261.561709	541.149309	18.945293	-0.049188	1.476226
261.338273	533.310557	18.950298	-0.049142	1.468686
261.293518	525.506695	18.955303	-0.049128	1.461170
261.025537	517.737432	18.960307	-0.049074	1.453612
261.166248	509.893877	18.965312	-0.049095	1.446008
261.213501	502.105089	18.970317	-0.049099	1.438402
261.027236	494.312481	18.975322	-0.049059	1.430714
260.924844	486.538584	18.980327	-0.049035	1.423017
260.591013	478.795631	18.985331	-0.048968	1.415271
260.589191	470.993557	18.990336	-0.048962	1.407478
260.561780	463.219286	18.995341	-0.048952	1.399665
260.303889	455.456574	19.000346	-0.048899	1.391781
260.139793	447.684797	19.005351	-0.048864	1.383859
260.025749	439.916693	19.010355	-0.048838	1.375903
260.015594	432.130059	19.015360	-0.048831	1.367900
259.976324	424.368426	19.020365	-0.048818	1.359870
259.902236	416.606864	19.025370	-0.048800	1.351787
259.752817	408.856055	19.030375	-0.048767	1.343653
259.669330	401.114974	19.035379	-0.048746	1.335492
259.791496	393.330494	19.040384	-0.048764	1.327271
259.469418	385.642831	19.045389	-0.048699	1.319022
259.179393	377.846748	19.050394	-0.048640	1.310611
259.079639	370.075305	19.055399	-0.048617	1.302206
258.931668	362.359753	19.060403	-0.048584	1.293799
258.975675	354.615138	19.065408	-0.048587	1.285340
258.855351	346.919749	19.070413	-0.048560	1.276849
258.650264	339.212818	19.075418	-0.048517	1.268273
258.436287	331.538029	19.080423	-0.048472	1.259672
258.102642	323.869326	19.085427	-0.048405	1.250996
257.989926	316.178328	19.090432	-0.048379	1.242277
257.947128	308.481667	19.095437	-0.048366	1.233503
257.556221	300.818180	19.100442	-0.048289	1.224636
257.410128	293.149610	19.105447	-0.048256	1.215746
256.852796	285.527461	19.110451	-0.048148	1.206764
256.518684	277.894682	19.115456	-0.048081	1.197746
256.277381	270.227843	19.120461	-0.048031	1.188638
256.062754	262.574257	19.125466	-0.047986	1.179481
255.552815	254.974531	19.130471	-0.047886	1.170256
255.058776	247.367732	19.135475	-0.047789	1.160953
254.914161	239.711114	19.140480	-0.047757	1.151586
254.573054	232.070957	19.145485	-0.047689	1.142121
254.056409	224.493339	19.150490	-0.047588	1.132617
253.729823	216.896078	19.155495	-0.047522	1.123049
253.338140	209.312070	19.160499	-0.047445	1.113401
252.937477	201.733643	19.165504	-0.047365	1.103674
252.491749	194.179072	19.170509	-0.047277	1.093881
252.118405	186.610014	19.175514	-0.047203	1.083996
251.911965	179.042537	19.180519	-0.047160	1.074060
251.468753	171.495055	19.185523	-0.047072	1.064004
251.102057	163.972635	19.190528	-0.046999	1.053903
250.859832	156.419431	19.195533	-0.046949	1.043691
250.135260	148.974033	19.200538	-0.046809	1.033411
249.936435	141.438815	19.205543	-0.046768	1.023029
249.411292	133.968619	19.210547	-0.046665	1.012553
248.814985	126.531315	19.215552	-0.046549	1.001995
248.341406	119.066875	19.220557	-0.046456	0.991317
247.881825	111.600283	19.225562	-0.046366	0.980522
247.515926	104.157170	19.230567	-0.046293	0.969665
246.933869	96.757782	19.235571	-0.046180	0.958694
246.726125	89.315623	19.240576	-0.046136	0.947629
246.146239	81.954506	19.245581	-0.046024	0.936457
245.649132	74.588298	19.250586	-0.045927	0.925164
245.087763	67.265859	19.255591	-0.045817	0.913782
244.719411	60.126986	19.260595	-0.045744	0.902595