Tue Mar 23 11:43:22 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.510059	0.085542	0.000000	0.000005	0.722624

0.477572	-0.033793	0.005005	0.000011	0.722378
0.460724	-0.026664	0.010010	0.000014	0.722387
0.225843	0.010856	0.015014	0.000058	0.722378
0.355827	-0.010022	0.020019	0.000034	0.722383
0.510597	-0.037975	0.025024	0.000005	0.722382
0.269198	0.002613	0.030029	0.000050	0.722378
0.576363	-0.046906	0.035034	-0.000008	0.722388
0.618909	-0.060047	0.040038	-0.000016	0.722377
0.380974	-0.013598	0.045043	0.000029	0.722385
0.490899	-0.033210	0.050048	0.000008	0.722386
0.489086	-0.036347	0.055053	0.000008	0.722379
0.476496	-0.030175	0.060058	0.000011	0.722387
0.327954	-0.008701	0.065062	0.000038	0.722377
0.342347	-0.009716	0.070067	0.000035	0.722380
0.508109	-0.039188	0.075072	0.000004	0.722381
0.448148	-0.091615	0.080077	0.000016	0.722257
0.782653	-0.236024	0.085082	-0.000047	0.722090
0.606808	-0.209489	0.090086	-0.000014	0.722081
0.675731	-0.219259	0.095091	-0.000027	0.722086
0.646604	-0.216221	0.100096	-0.000022	0.722082
0.633866	-0.215466	0.105101	-0.000019	0.722079
0.480508	-0.242700	0.110106	0.000009	0.721972
0.491567	-0.357883	0.115110	0.000007	0.721750
0.331045	-0.327323	0.120115	0.000037	0.721754
0.635289	-0.381530	0.125120	-0.000020	0.721754
0.601216	-0.378048	0.130125	-0.000014	0.721749
0.466451	-0.413449	0.135130	0.000011	0.721632
0.501202	-0.514065	0.140134	0.000005	0.721447
0.398492	-0.493600	0.145139	0.000024	0.721451
0.460563	-0.507828	0.150144	0.000012	0.721445
0.499643	-0.547767	0.155149	0.000005	0.721381
0.437987	-0.662367	0.160154	0.000016	0.721134
0.302245	-0.643042	0.165158	0.000042	0.721124
0.314398	-0.643146	0.170163	0.000039	0.721129
0.346410	-0.693791	0.175168	0.000033	0.721040
0.362174	-0.776039	0.180173	0.000030	0.720884
0.326509	-0.766043	0.185178	0.000037	0.720891
0.271765	-0.760622	0.190182	0.000047	0.720883
0.271989	-0.917111	0.195187	0.000047	0.720575
0.207599	-0.917700	0.200192	0.000059	0.720552
0.584548	-0.987116	0.205197	-0.000011	0.720547
0.699871	-1.132488	0.210202	-0.000033	0.720302
0.322441	-1.103445	0.215206	0.000037	0.720227
0.443797	-1.121648	0.220211	0.000015	0.720234
0.453854	-1.280738	0.225216	0.000013	0.719924
0.214337	-1.248510	0.230221	0.000057	0.719903
0.486690	-1.327459	0.235226	0.000007	0.719843
0.313228	-1.415589	0.240230	0.000039	0.719609
0.356750	-1.422193	0.245235	0.000031	0.719611
0.204691	-1.503371	0.250240	0.000059	0.719398
-0.005607	-1.529399	0.255245	0.000098	0.719273
-0.019086	-1.532027	0.260250	0.000100	0.719263
0.137831	-1.711517	0.265254	0.000071	0.718964
0.036604	-1.691636	0.270259	0.000090	0.718968
0.047092	-1.795254	0.275264	0.000088	0.718768
0.111804	-1.867902	0.280269	0.000076	0.718647
0.176311	-1.922203	0.285274	0.000064	0.718563
0.014170	-1.996209	0.290278	0.000094	0.718360
-0.044447	-1.999486	0.295283	0.000105	0.718333
-0.316503	-2.104565	0.300288	0.000155	0.718030
-0.430831	-2.086223	0.305293	0.000177	0.718026
-0.148442	-2.263319	0.310298	0.000124	0.717775
-0.304719	-2.269486	0.315302	0.000153	0.717708
-0.512495	-2.337727	0.320307	0.000192	0.717500
-1.036276	-2.300060	0.325312	0.000289	0.717391
-1.621892	-2.253699	0.330317	0.000398	0.717276
-3.204678	-2.062759	0.335322	0.000693	0.717096
-3.209311	-2.067617	0.340326	0.000693	0.717085
-3.225541	-2.104881	0.345331	0.000696	0.717006
-4.140636	-2.065611	0.350336	0.000867	0.716761
-3.971557	-2.097736	0.355341	0.000835	0.716758
-4.018240	-2.083354	0.360346	0.000844	0.716770
-4.423262	-2.146467	0.365350	0.000919	0.716502
-5.162795	-2.036989	0.370355	0.001057	0.716458
-5.211751	-2.027367	0.375360	0.001066	0.716460
-4.784188	-2.105882	0.380365	0.000986	0.716456
-5.282014	-2.162132	0.385370	0.001079	0.716169
-6.222857	-2.010209	0.390374	0.001254	0.716138
-5.819761	-2.078853	0.395379	0.001179	0.716144
-5.449054	-2.145667	0.400384	0.001109	0.716143
-6.140498	-2.121651	0.405389	0.001238	0.715947
-6.657134	-2.054802	0.410394	0.001334	0.715897
-6.459662	-2.094661	0.415398	0.001297	0.715888
-6.467921	-2.091068	0.420403	0.001299	0.715892
-6.529576	-2.127218	0.425408	0.001310	0.715799
-7.777945	-2.032174	0.430413	0.001543	0.715547
-7.171474	-2.133033	0.435418	0.001430	0.715561
-7.646200	-2.054741	0.440422	0.001518	0.715549
-7.594420	-2.060819	0.445427	0.001508	0.715555
-7.402804	-2.133241	0.450432	0.001472	0.715479
-8.803048	-2.006362	0.455437	0.001733	0.715236
-8.357580	-2.080713	0.460442	0.001650	0.715247
-8.742622	-2.016541	0.465446	0.001722	0.715238
-8.680202	-2.026601	0.470451	0.001710	0.715240
-8.672177	-2.028073	0.475456	0.001708	0.715240
-8.638444	-2.090646	0.480461	0.001702	0.715128
-9.460084	-2.048984	0.485466	0.001855	0.714921
-9.600414	-2.026981	0.490470	0.001881	0.714915
-9.887915	-1.972434	0.495475	0.001934	0.714922
-9.272536	-2.083698	0.500480	0.001820	0.714918
-9.423810	-2.058055	0.505485	0.001848	0.714916
-9.634171	-2.041742	0.510490	0.001887	0.714874
-10.360629	-2.045053	0.515494	0.002022	0.714611
-9.990242	-2.109222	0.520499	0.001953	0.714615
-10.312458	-2.051165	0.525504	0.002013	0.714616
-10.452366	-2.029196	0.530509	0.002039	0.714610
-9.991489	-2.108264	0.535514	0.001953	0.714617
-10.419422	-2.035464	0.540518	0.002032	0.714610
-10.816714	-2.124184	0.545523	0.002106	0.714293
-11.144149	-2.067553	0.550528	0.002167	0.714290
-11.718530	-1.969527	0.555533	0.002274	0.714282
-11.248433	-2.049299	0.560538	0.002187	0.714290
-11.273905	-2.049950	0.565542	0.002191	0.714280
-11.377333	-2.029253	0.570547	0.002210	0.714284
-11.428673	-2.052321	0.575552	0.002220	0.714220
-12.393697	-2.006839	0.580557	0.002399	0.713969
-11.959526	-2.079666	0.585562	0.002319	0.713979
-12.515231	-1.985434	0.590566	0.002422	0.713969
-12.686448	-1.952308	0.595571	0.002454	0.713975
-12.022724	-2.070029	0.600576	0.002330	0.713976
-12.328771	-2.019012	0.605581	0.002387	0.713969
-12.414271	-1.998839	0.610586	0.002403	0.713979
-12.843282	-2.077479	0.615590	0.002483	0.713671
-12.891154	-2.075274	0.620595	0.002491	0.713658
-12.786509	-2.093604	0.625600	0.002472	0.713659
-13.116962	-2.037295	0.630605	0.002533	0.713654
-13.015369	-2.052020	0.635610	0.002514	0.713661
-12.984098	-2.062225	0.640614	0.002508	0.713652
-13.145576	-2.087187	0.645619	0.002538	0.713545
-14.256242	-1.979462	0.650624	0.002745	0.713366
-13.861859	-2.051367	0.655629	0.002672	0.713363
-13.962760	-2.029356	0.660634	0.002690	0.713371
-14.184928	-1.993118	0.665638	0.002731	0.713365
-13.939150	-2.036433	0.670643	0.002686	0.713366
-14.076671	-2.010567	0.675648	0.002711	0.713369
-14.142484	-2.025717	0.680653	0.002723	0.713316
-14.511157	-2.101347	0.685658	0.002792	0.713034
-14.830517	-2.049047	0.690662	0.002851	0.713026
-15.307589	-1.962928	0.695667	0.002940	0.713028
-14.914567	-2.031494	0.700672	0.002867	0.713031
-14.813266	-2.052838	0.705677	0.002848	0.713025
-14.742042	-2.061295	0.710682	0.002834	0.713033
-15.141090	-2.007503	0.715686	0.002909	0.712999
-15.818018	-2.029209	0.720691	0.003035	0.712716
-15.668260	-2.053148	0.725696	0.003007	0.712721
-16.315161	-1.942025	0.730701	0.003127	0.712713
-15.753451	-2.035276	0.735706	0.003022	0.712727
-15.917699	-2.013387	0.740710	0.003053	0.712713
-16.069445	-1.983851	0.745715	0.003081	0.712718
-16.145475	-1.970859	0.750720	0.003095	0.712717
-16.123916	-2.047081	0.755725	0.003091	0.712573
-16.890727	-1.996788	0.760730	0.003234	0.712401
-16.993218	-1.982725	0.765734	0.003253	0.712393
-16.878546	-2.002139	0.770739	0.003231	0.712395
-16.593592	-2.050909	0.775744	0.003178	0.712399
-16.808349	-2.018452	0.780749	0.003218	0.712388
-16.696137	-2.034764	0.785754	0.003197	0.712395
-16.666987	-2.085398	0.790758	0.003192	0.712305
-17.721890	-2.002892	0.795763	0.003388	0.712095
-17.511869	-2.039137	0.800768	0.003349	0.712097
-17.829147	-1.985632	0.805773	0.003408	0.712091
-17.549652	-2.031043	0.810778	0.003355	0.712100
-17.991272	-1.957736	0.815782	0.003438	0.712090
-17.901921	-1.971270	0.820787	0.003421	0.712095
-17.534080	-2.042208	0.825792	0.003352	0.712084
-18.559704	-2.021319	0.830797	0.003543	0.711762
-18.674821	-1.995414	0.835802	0.003565	0.711773
-18.565563	-2.018366	0.840806	0.003544	0.711766
-18.492215	-2.031085	0.845811	0.003530	0.711767
-18.521609	-2.024600	0.850816	0.003536	0.711769
-18.682109	-2.001489	0.855821	0.003566	0.711759
-18.421467	-2.042057	0.860826	0.003517	0.711770
-18.845404	-2.109000	0.865830	0.003596	0.711486
-19.621186	-1.985343	0.870835	0.003740	0.711457
-19.253087	-2.049598	0.875840	0.003672	0.711460
-19.595189	-1.992252	0.880845	0.003735	0.711453
-19.578161	-1.990947	0.885850	0.003732	0.711462
-19.298608	-2.043612	0.890854	0.003680	0.711457
-19.501884	-2.007205	0.895859	0.003718	0.711457
-19.938598	-2.068636	0.900864	0.003799	0.711179
-20.581302	-1.974114	0.905869	0.003918	0.711140
-20.166305	-2.045006	0.910874	0.003841	0.711146
-20.580218	-1.974980	0.915878	0.003918	0.711139
-20.800314	-1.934598	0.920883	0.003959	0.711141
-20.298416	-2.019877	0.925888	0.003865	0.711150
-20.454856	-1.997444	0.930893	0.003894	0.711139
-20.458252	-2.065652	0.935898	0.003895	0.711002
-21.307295	-1.976418	0.940902	0.004053	0.710878
-21.246382	-1.988292	0.945907	0.004041	0.710876
-21.168408	-2.001602	0.950912	0.004027	0.710877
-21.437015	-1.956993	0.955917	0.004077	0.710871
-20.970154	-2.034822	0.960922	0.003990	0.710882
-21.490079	-1.947000	0.965926	0.004086	0.710873
-21.291966	-2.056749	0.970931	0.004050	0.710724
-21.983880	-2.025876	0.975936	0.004178	0.710540
-22.340454	-1.965553	0.980941	0.004245	0.710533
-22.293545	-1.970477	0.985946	0.004236	0.710540
-22.149890	-1.997678	0.990950	0.004209	0.710537
-21.974544	-2.027674	0.995955	0.004176	0.710540
-22.437145	-1.943302	1.000960	0.004262	0.710544
-22.597678	-1.938884	1.005965	0.004292	0.710496
-22.747512	-2.047400	1.010970	0.004320	0.710226
-23.166484	-1.976971	1.015974	0.004398	0.710218
-23.638789	-1.891143	1.020979	0.004486	0.710221
-22.857411	-2.029549	1.025984	0.004340	0.710223
-23.230218	-1.965588	1.030989	0.004409	0.710218
-23.154008	-1.974759	1.035994	0.004395	0.710227
-22.713852	-2.055336	1.040998	0.004313	0.710223
-23.317486	-2.101676	1.046003	0.004425	0.709915
-23.936843	-1.999012	1.051008	0.004541	0.709900
-24.389308	-1.922221	1.056013	0.004625	0.709893
-23.514662	-2.073503	1.061018	0.004462	0.709902
-24.057447	-1.979292	1.066022	0.004563	0.709897
-24.157826	-1.960630	1.071027	0.004581	0.709899
-23.724062	-2.041473	1.076032	0.004501	0.709892
-24.579779	-2.036499	1.081037	0.004660	0.709597
-24.995942	-1.959151	1.086042	0.004737	0.709604
-24.808115	-1.994027	1.091046	0.004702	0.709601
-24.673677	-2.017947	1.096051	0.004677	0.709601
-24.908558	-1.974968	1.101056	0.004721	0.709604
-25.229986	-1.921366	1.106061	0.004780	0.709596
-24.777966	-1.997387	1.111066	0.004696	0.709606
-25.305071	-2.031520	1.116070	0.004794	0.709350
-26.261347	-1.903047	1.121075	0.004972	0.709266
-25.435918	-2.047715	1.126080	0.004819	0.709271
-25.583976	-2.024690	1.131085	0.004846	0.709264
-26.032047	-1.941228	1.136090	0.004929	0.709272
-25.971212	-1.954060	1.141094	0.004918	0.709268
-25.889056	-1.968509	1.146099	0.004902	0.709268
-25.857186	-2.032090	1.151104	0.004897	0.709153
-27.114031	-1.904962	1.156109	0.005130	0.708959
-26.351455	-2.037226	1.161114	0.004988	0.708966
-26.722643	-1.973583	1.166118	0.005057	0.708961
-26.923721	-1.937250	1.171123	0.005095	0.708963
-26.683488	-1.977645	1.176128	0.005050	0.708968
-26.687269	-1.982588	1.181133	0.005051	0.708957
-26.948699	-1.938814	1.186138	0.005099	0.708951
-27.388602	-2.015315	1.191142	0.005181	0.708641
-27.530460	-1.989885	1.196147	0.005207	0.708641
-27.858121	-1.930372	1.201152	0.005268	0.708644
-27.760414	-1.950085	1.206157	0.005250	0.708639
-27.299592	-2.027843	1.211162	0.005164	0.708648
-27.617923	-1.974979	1.216166	0.005223	0.708641
-27.634171	-1.971503	1.221171	0.005226	0.708642
-27.581749	-2.105914	1.226176	0.005216	0.708392
-28.368905	-1.985897	1.231181	0.005363	0.708351
-28.472536	-1.964281	1.236186	0.005382	0.708358
-28.529155	-1.956571	1.241190	0.005392	0.708353
-28.224376	-2.010225	1.246195	0.005336	0.708355
-28.120569	-2.026897	1.251200	0.005316	0.708358
-28.557732	-1.994633	1.256205	0.005398	0.708267
-29.551480	-1.940598	1.261210	0.005582	0.708020
-28.990610	-2.043432	1.266214	0.005478	0.708015
-29.583917	-1.937512	1.271219	0.005588	0.708015
-29.459504	-1.956379	1.276224	0.005565	0.708022
-29.294594	-1.990325	1.281229	0.005534	0.708013
-29.391692	-1.968901	1.286234	0.005552	0.708022
-29.279382	-1.996275	1.291238	0.005531	0.708007
-29.652015	-2.081120	1.296243	0.005601	0.707704
-30.297807	-1.964173	1.301248	0.005721	0.707708
-30.864320	-1.869522	1.306253	0.005826	0.707695
-30.081216	-2.001535	1.311258	0.005680	0.707711
-30.018283	-2.016761	1.316262	0.005668	0.707703
-30.693650	-1.896099	1.321267	0.005794	0.707703
-30.280381	-1.968895	1.326272	0.005717	0.707705
-30.339113	-2.075197	1.331277	0.005728	0.707471
-31.305824	-1.946087	1.336282	0.005908	0.707385
-31.282098	-1.953780	1.341286	0.005903	0.707378
-31.036082	-1.996111	1.346291	0.005857	0.707381
-30.823245	-2.032140	1.351296	0.005818	0.707385
-31.112930	-1.984135	1.356301	0.005872	0.707378
-30.931976	-2.012072	1.361306	0.005838	0.707387
-31.340708	-2.072308	1.366310	0.005914	0.707120
-32.007285	-1.970193	1.371315	0.006038	0.707086
-31.997037	-1.969575	1.376320	0.006036	0.707092
-32.095661	-1.955657	1.381325	0.006054	0.707084
-31.927559	-1.980995	1.386330	0.006023	0.707094
-32.023903	-1.964956	1.391334	0.006041	0.707092
-32.134962	-1.945246	1.396339	0.006061	0.707092
-32.270496	-2.055431	1.401344	0.006086	0.706822
-33.072667	-1.945612	1.406349	0.006236	0.706756
-32.822261	-1.986476	1.411354	0.006189	0.706763
-32.550717	-2.038565	1.416358	0.006138	0.706756
-33.001325	-1.957874	1.421363	0.006222	0.706757
-32.821187	-1.987574	1.426368	0.006188	0.706762
-32.794268	-1.994940	1.431373	0.006183	0.706757
-33.077404	-2.079996	1.436378	0.006236	0.706485
-33.858253	-1.959707	1.441382	0.006381	0.706447
-34.147100	-1.907223	1.446387	0.006435	0.706449
-33.357018	-2.047456	1.451392	0.006288	0.706451
-33.798460	-1.971387	1.456397	0.006370	0.706446
-33.942949	-1.941059	1.461402	0.006397	0.706455
-33.858699	-1.960388	1.466406	0.006381	0.706446
-34.156495	-2.025261	1.471411	0.006436	0.706209
-34.714134	-1.962287	1.476416	0.006540	0.706136
-34.669238	-1.973864	1.481421	0.006532	0.706129
-34.424495	-2.013568	1.486426	0.006486	0.706137
-34.506706	-2.002181	1.491430	0.006501	0.706131
-34.536679	-1.995990	1.496435	0.006507	0.706133
-34.416708	-2.015436	1.501440	0.006484	0.706137
-35.195863	-2.000204	1.506445	0.006629	0.705888
-35.472853	-1.958561	1.511450	0.006681	0.705873
-35.498326	-1.957324	1.516454	0.006685	0.705867
-35.465856	-1.961952	1.521459	0.006679	0.705869
-35.621020	-1.931858	1.526464	0.006708	0.705874
-35.662343	-1.930239	1.531469	0.006716	0.705863
-35.177287	-2.011768	1.536474	0.006625	0.705873
-35.760206	-2.055117	1.541478	0.006734	0.705577
-36.474552	-1.952115	1.546483	0.006867	0.705528
-36.192962	-2.000021	1.551488	0.006814	0.705533
-36.091299	-2.022643	1.556493	0.006795	0.705524
-36.430731	-1.958195	1.561498	0.006858	0.705532
-36.616661	-1.928821	1.566502	0.006893	0.705524
-36.243871	-1.994572	1.571507	0.006823	0.705526
-36.750760	-2.053565	1.576512	0.006918	0.705226
-37.305924	-1.963145	1.581517	0.007021	0.705208
-37.254070	-1.969020	1.586522	0.007011	0.705215
-37.195951	-1.983376	1.591526	0.007000	0.705208
-37.117819	-1.996066	1.596531	0.006986	0.705210
-36.740300	-2.060995	1.601536	0.006915	0.705215
-37.068730	-2.050286	1.606541	0.006976	0.705119
-37.905006	-2.014295	1.611546	0.007132	0.704891
-37.714222	-2.050862	1.616550	0.007096	0.704886
-37.815162	-2.032836	1.621555	0.007115	0.704887
-38.109737	-1.976345	1.626560	0.007170	0.704895
-38.136521	-1.975566	1.631565	0.007175	0.704887
-37.818298	-2.027643	1.636570	0.007115	0.704896
-38.013366	-2.081311	1.641574	0.007152	0.704718
-39.262723	-1.921902	1.646579	0.007384	0.704591
-38.821031	-1.998120	1.651584	0.007302	0.704596
-38.825060	-2.000698	1.656589	0.007302	0.704590
-39.045581	-1.956633	1.661594	0.007343	0.704600
-38.980770	-1.972450	1.666598	0.007331	0.704591
-39.003189	-1.969698	1.671603	0.007335	0.704589
-38.966674	-2.040058	1.676608	0.007328	0.704460
-40.026093	-1.949158	1.681613	0.007526	0.704263
-39.660785	-2.011221	1.686618	0.007458	0.704269
-40.084838	-1.937303	1.691622	0.007536	0.704266
-40.160563	-1.925358	1.696627	0.007550	0.704263
-39.464493	-2.047966	1.701632	0.007421	0.704266
-39.640504	-2.018920	1.706637	0.007453	0.704262
-39.992385	-2.004461	1.711642	0.007519	0.704164
-40.777663	-1.967989	1.716646	0.007665	0.703956
-40.467632	-2.023181	1.721651	0.007607	0.703956
-40.742743	-1.970935	1.726656	0.007658	0.703963
-40.958491	-1.938711	1.731661	0.007698	0.703950
-40.556772	-2.006339	1.736666	0.007623	0.703959
-40.766822	-1.972035	1.741670	0.007662	0.703952
-41.166519	-1.909690	1.746675	0.007737	0.703935
-41.314076	-2.028041	1.751680	0.007764	0.703643
-41.614395	-1.978224	1.756685	0.007820	0.703636
-41.911061	-1.921479	1.761690	0.007875	0.703644
-41.613414	-1.977790	1.766694	0.007820	0.703637
-41.617326	-1.977252	1.771699	0.007820	0.703637
-41.598901	-1.976597	1.776704	0.007817	0.703645
-41.760425	-1.952914	1.781709	0.007847	0.703635
-41.903731	-2.046177	1.786714	0.007873	0.703395
-42.623662	-1.942931	1.791718	0.008007	0.703345
-42.786991	-1.916024	1.796723	0.008038	0.703340
-42.089508	-2.037194	1.801728	0.007908	0.703347
-42.351712	-1.994594	1.806733	0.007957	0.703339
-42.478152	-1.967499	1.811738	0.007980	0.703348
-42.390337	-1.986559	1.816742	0.007964	0.703341
-42.961509	-2.051442	1.821747	0.008070	0.703005
-43.192413	-2.005070	1.826752	0.008113	0.703016
-43.647625	-1.928485	1.831757	0.008197	0.703007
-42.930278	-2.052891	1.836762	0.008064	0.703014
-42.906223	-2.059927	1.841766	0.008059	0.703008
-43.661123	-1.926711	1.846771	0.008200	0.703006
-43.332463	-2.021617	1.851776	0.008138	0.702933
-44.189711	-1.988138	1.856781	0.008298	0.702692
-44.124533	-1.994704	1.861786	0.008286	0.702702
-44.508492	-1.927458	1.866790	0.008357	0.702700
-44.287707	-1.970104	1.871795	0.008316	0.702693
-43.915224	-2.033345	1.876800	0.008246	0.702700
-44.524884	-1.927833	1.881805	0.008360	0.702693
-44.182017	-2.004560	1.886810	0.008296	0.702662
-44.901012	-2.021035	1.891814	0.008430	0.702370
-45.377024	-1.936257	1.896819	0.008518	0.702370
-45.219991	-1.960783	1.901824	0.008489	0.702377
-44.932525	-2.015471	1.906829	0.008435	0.702370
-44.975255	-2.005041	1.911834	0.008443	0.702376
-45.277000	-1.951754	1.916838	0.008499	0.702375
-44.887915	-2.034322	1.921843	0.008427	0.702349
-45.421259	-2.070284	1.926848	0.008526	0.702084
-46.086698	-1.956633	1.931853	0.008650	0.702074
-46.196550	-1.933428	1.936858	0.008670	0.702081
-45.836348	-2.000310	1.941862	0.008603	0.702076
-46.197680	-1.938059	1.946867	0.008670	0.702072
-46.273654	-1.919736	1.951872	0.008684	0.702082
-46.091749	-1.956260	1.956877	0.008650	0.702074
-46.456503	-2.032709	1.961882	0.008718	0.701787
-47.064149	-1.945166	1.966886	0.008831	0.701746
-47.182234	-1.925623	1.971891	0.008853	0.701743
-46.534362	-2.037160	1.976896	0.008732	0.701751
-47.097703	-1.942130	1.981901	0.008837	0.701740
-46.982106	-1.958117	1.986906	0.008816	0.701750
-46.805980	-1.991103	1.991910	0.008783	0.701747
-47.341636	-2.011999	1.996915	0.008882	0.701511
-47.952193	-1.938530	2.001920	0.008996	0.701440

-47.914450	-1.943918	2.011917	0.008989	0.701443
-47.569543	-2.006153	2.021914	0.008924	0.701441
-47.915508	-1.945911	2.031910	0.008989	0.701439
-47.673782	-1.989712	2.041907	0.008943	0.701438
-47.837270	-1.959802	2.051904	0.008974	0.701440
-47.560020	-2.009396	2.061901	0.008922	0.701440
-47.812628	-1.963251	2.071898	0.008969	0.701442
-47.923453	-1.945201	2.081894	0.008989	0.701439
-47.937993	-1.942310	2.091891	0.008992	0.701440
-47.948909	-1.940412	2.101888	0.008994	0.701440
-47.762562	-1.974340	2.111885	0.008959	0.701439
-47.735674	-1.979337	2.121882	0.008954	0.701439
-47.872846	-1.894376	2.131878	0.008979	0.701562
-46.851918	-1.984680	2.141875	0.008789	0.701748
-46.902977	-1.976900	2.151872	0.008798	0.701746
-46.747241	-2.003516	2.161869	0.008769	0.701748
-46.978548	-1.963099	2.171866	0.008812	0.701747
-46.869874	-1.916188	2.181862	0.008791	0.701881
-45.869917	-1.999035	2.191859	0.008605	0.702075
-46.062042	-1.963866	2.201856	0.008641	0.702077
-46.036564	-1.967183	2.211853	0.008636	0.702080
-45.828560	-1.996665	2.221850	0.008597	0.702096
-45.583579	-1.903848	2.231846	0.008551	0.702372
-45.154909	-1.980510	2.241843	0.008471	0.702372
-45.388989	-1.938519	2.251840	0.008514	0.702373
-45.064121	-1.933758	2.261837	0.008454	0.702500
-44.557505	-1.927479	2.271834	0.008359	0.702695
-44.428062	-1.950835	2.281830	0.008335	0.702695
-44.637469	-1.914056	2.291827	0.008374	0.702694
-43.738784	-1.926665	2.301824	0.008206	0.702993
-43.440794	-1.973530	2.311821	0.008151	0.703006
-43.248871	-2.005780	2.321818	0.008115	0.703010
-43.445916	-1.953334	2.331814	0.008151	0.703046
-42.537399	-1.968194	2.341811	0.007982	0.703343
-42.579445	-1.961057	2.351808	0.007990	0.703343
-42.430129	-1.987684	2.361805	0.007962	0.703343
-42.446203	-1.919380	2.371802	0.007964	0.703475
-41.463787	-2.015967	2.381798	0.007781	0.703634
-41.726274	-1.969109	2.391795	0.007830	0.703635
-41.746129	-1.965463	2.401792	0.007834	0.703635
-41.068663	-1.960459	2.411789	0.007707	0.703889
-40.960774	-1.946971	2.421786	0.007687	0.703956
-40.757594	-1.985715	2.431782	0.007649	0.703951
-40.666986	-1.959652	2.441779	0.007632	0.704037
-39.869944	-1.989719	2.451776	0.007483	0.704263
-39.846215	-1.993532	2.461773	0.007479	0.704264
-39.875718	-1.988399	2.471770	0.007484	0.704264
-39.268916	-1.989555	2.481766	0.007371	0.704480
-39.052668	-1.975385	2.491763	0.007330	0.704587
-38.952569	-1.992151	2.501760	0.007312	0.704589
-38.872071	-2.004996	2.511757	0.007296	0.704593
-38.656644	-1.901546	2.521754	0.007256	0.704879
-38.063205	-2.001629	2.531750	0.007146	0.704891
-38.282325	-1.963940	2.541747	0.007186	0.704888
-37.794068	-1.948286	2.551744	0.007095	0.705095
-37.474484	-1.947789	2.561741	0.007035	0.705211
-37.389835	-1.962536	2.571738	0.007019	0.705212
-37.249021	-1.949300	2.581734	0.006993	0.705290
-36.582232	-1.950688	2.591731	0.006869	0.705527
-36.369805	-1.987899	2.601728	0.006829	0.705528
-36.510423	-1.964010	2.611725	0.006855	0.705526
-35.863454	-1.944306	2.621722	0.006734	0.705798
-35.419660	-1.991405	2.631718	0.006652	0.705863
-35.635018	-1.952837	2.641715	0.006691	0.705864
-35.317479	-1.988347	2.651712	0.006632	0.705907
-34.905723	-1.949648	2.661709	0.006555	0.706132
-34.513639	-2.020858	2.671706	0.006482	0.706130
-34.760180	-1.977782	2.681702	0.006528	0.706129
-34.262979	-1.945721	2.691699	0.006435	0.706372
-33.770449	-1.996732	2.701696	0.006343	0.706446
-33.772283	-1.995676	2.711693	0.006343	0.706448
-33.861799	-1.938944	2.721690	0.006360	0.706530
-32.818649	-2.013054	2.731686	0.006166	0.706755
-33.187765	-1.948408	2.741683	0.006234	0.706753
-33.038164	-1.974222	2.751680	0.006206	0.706755
-32.376270	-1.946726	2.761677	0.006083	0.707047
-31.901331	-2.012930	2.771674	0.005994	0.707085
-32.093989	-1.979072	2.781670	0.006030	0.707084
-32.052065	-1.934790	2.791667	0.006022	0.707188
-31.107862	-2.009136	2.801664	0.005846	0.707377
-31.326611	-1.969538	2.811661	0.005886	0.707379
-31.284514	-1.975920	2.821658	0.005878	0.707381
-30.455167	-1.976917	2.831654	0.005724	0.707676
-30.394914	-1.975744	2.841651	0.005712	0.707701
-30.225549	-2.005740	2.851648	0.005681	0.707701
-30.113307	-1.972812	2.861645	0.005660	0.707808
-29.414889	-1.993093	2.871642	0.005529	0.708017
-29.674097	-1.948118	2.881638	0.005577	0.708015
-29.568616	-1.967625	2.891635	0.005558	0.708014
-28.721722	-1.958973	2.901632	0.005400	0.708334
-28.571629	-1.976136	2.911629	0.005372	0.708354
-28.436814	-1.999818	2.921626	0.005346	0.708355
-28.509627	-1.933627	2.931622	0.005360	0.708462
-27.840003	-1.964468	2.941619	0.005235	0.708639
-27.691253	-1.990788	2.951616	0.005207	0.708640
-27.667900	-1.993866	2.961613	0.005203	0.708643
-26.885555	-1.989087	2.971610	0.005057	0.708932
-27.081728	-1.940208	2.981606	0.005093	0.708960
-26.816112	-1.989771	2.991603	0.005043	0.708956
-26.624010	-1.952199	3.001600	0.005007	0.709100
-25.838415	-2.007754	3.011597	0.004861	0.709269
-25.879249	-2.000291	3.021594	0.004868	0.709270
-26.040137	-1.972763	3.031590	0.004898	0.709268
-25.292918	-1.956352	3.041587	0.004759	0.709568
-25.110352	-1.973111	3.051584	0.004725	0.709599
-25.115238	-1.971545	3.061581	0.004725	0.709601
-24.816644	-1.960418	3.071578	0.004670	0.709730
-24.430689	-1.945228	3.081574	0.004598	0.709898
-24.090612	-2.007550	3.091571	0.004534	0.709895
-24.375479	-1.953830	3.101568	0.004587	0.709902
-23.611056	-1.928571	3.111565	0.004445	0.710225
-23.187558	-2.004193	3.121562	0.004366	0.710225
-23.430044	-1.962559	3.131558	0.004411	0.710222
-23.061118	-1.943489	3.141555	0.004342	0.710392
-22.557771	-1.961255	3.151552	0.004248	0.710536
-22.392600	-1.990379	3.161549	0.004217	0.710537
-22.225145	-2.020770	3.171546	0.004186	0.710536
-21.689248	-1.957963	3.181542	0.004086	0.710852
-21.274975	-2.022662	3.191539	0.004008	0.710871
-21.572423	-1.968305	3.201536	0.004063	0.710874
-21.474999	-1.948373	3.211533	0.004045	0.710949
-20.710492	-1.986768	3.221530	0.003903	0.711144
-20.878424	-1.957326	3.231526	0.003934	0.711144
-20.695105	-1.992500	3.241523	0.003899	0.711139
-20.170866	-1.940514	3.251520	0.003802	0.711430
-19.772662	-1.996856	3.261517	0.003727	0.711459
-19.783577	-1.995037	3.271514	0.003729	0.711459
-19.616950	-1.965346	3.281510	0.003698	0.711578
-18.831025	-2.012945	3.291507	0.003551	0.711763
-19.230960	-1.941232	3.301504	0.003626	0.711764
-18.999968	-1.975025	3.311501	0.003583	0.711779
-18.230666	-1.953579	3.321498	0.003439	0.712095
-18.178471	-1.963317	3.331494	0.003429	0.712095
-18.096798	-1.978384	3.341491	0.003414	0.712094
-17.799101	-1.943950	3.351488	0.003358	0.712269
-17.208836	-1.989500	3.361485	0.003248	0.712388
-17.231748	-1.983229	3.371482	0.003252	0.712392
-17.099581	-2.002546	3.381478	0.003228	0.712401
-16.652599	-1.925727	3.391475	0.003144	0.712713
-16.397685	-1.970046	3.401472	0.003096	0.712716
-16.254007	-1.994982	3.411469	0.003070	0.712717
-15.861868	-1.968222	3.421466	0.002996	0.712910
-15.722588	-1.933294	3.431462	0.002970	0.713029
-15.512227	-1.970893	3.441459	0.002931	0.713029
-15.721996	-1.893525	3.451456	0.002970	0.713109
-14.309303	-2.015160	3.461453	0.002707	0.713368
-14.652009	-1.955651	3.471450	0.002770	0.713366
-14.447086	-1.992712	3.481446	0.002732	0.713365
-14.174562	-1.949696	3.491443	0.002681	0.713547
-13.692031	-1.979627	3.501440	0.002591	0.713659
-13.919149	-1.938352	3.511437	0.002633	0.713661
-13.526040	-1.994277	3.521434	0.002560	0.713689
-12.875031	-1.967964	3.531430	0.002438	0.713973
-12.857110	-1.970888	3.541427	0.002435	0.713973
-12.939728	-1.956021	3.551424	0.002450	0.713974
-12.307296	-1.973137	3.561421	0.002332	0.714164
-11.968874	-1.972781	3.571418	0.002269	0.714285
-11.992386	-1.970016	3.581414	0.002273	0.714283
-12.144719	-1.923537	3.591411	0.002301	0.714321
-10.969034	-1.986766	3.601408	0.002082	0.714612
-10.827066	-2.012572	3.611405	0.002056	0.714611
-10.944864	-1.990495	3.621402	0.002077	0.714614
-10.929655	-1.937132	3.631398	0.002074	0.714726
-10.122771	-1.986508	3.641395	0.001924	0.714913
-9.951279	-2.018084	3.651392	0.001892	0.714912
-10.143132	-1.983840	3.661389	0.001927	0.714912
-9.638127	-1.944724	3.671386	0.001833	0.715168
-9.239322	-1.982090	3.681382	0.001759	0.715236
-9.447970	-1.945446	3.691379	0.001797	0.715235
-8.867066	-2.005827	3.701376	0.001689	0.715321
-8.218821	-2.005817	3.711373	0.001568	0.715550
-7.888992	-2.062638	3.721370	0.001507	0.715554
-7.720111	-2.094694	3.731366	0.001475	0.715551
-7.937464	-2.035182	3.741363	0.001515	0.715592
-6.949885	-2.061735	3.751360	0.001331	0.715889
-6.760548	-2.096094	3.761357	0.001296	0.715888
-6.715191	-2.103509	3.771354	0.001287	0.715889
-6.786553	-2.092146	3.781350	0.001300	0.715887
-6.534894	-2.038438	3.791347	0.001253	0.716083
-6.055699	-2.097682	3.801344	0.001164	0.716135
-6.187589	-2.074475	3.811341	0.001188	0.716134
-6.147753	-2.056295	3.821338	0.001181	0.716185
-5.085792	-2.110716	3.831334	0.000983	0.716452
-5.219927	-2.087701	3.841331	0.001008	0.716451
-5.123549	-2.103846	3.851328	0.000990	0.716453
-5.188478	-2.031993	3.861325	0.001001	0.716573
-3.992544	-2.150735	3.871322	0.000779	0.716760
-4.426466	-2.072516	3.881318	0.000859	0.716762
-4.434584	-2.073011	3.891315	0.000861	0.716758
-3.812589	-2.049983	3.901312	0.000745	0.717023
-3.457214	-2.081368	3.911309	0.000678	0.717087
-3.247527	-2.117730	3.921306	0.000639	0.717089
-3.147377	-2.123802	3.931302	0.000620	0.717113
-2.807558	-2.048356	3.941299	0.000557	0.717382
-2.316230	-2.136374	3.951296	0.000465	0.717381
-2.578230	-2.087075	3.961293	0.000514	0.717387
-2.403661	-2.033091	3.971290	0.000481	0.717555
-1.991491	-2.030214	3.981286	0.000404	0.717707
-1.876926	-2.050820	3.991283	0.000383	0.717707
-1.797246	-2.010381	4.001280	0.000368	0.717815
-1.524976	-1.954286	4.011277	0.000317	0.718022
-1.243961	-2.003978	4.021274	0.000264	0.718023
-1.364374	-1.912338	4.031270	0.000286	0.718162
-1.391353	-1.810024	4.041267	0.000291	0.718355
-1.489815	-1.782921	4.051264	0.000309	0.718374
-1.330544	-1.673254	4.061261	0.000279	0.718647
-1.208854	-1.693940	4.071258	0.000257	0.718649
-1.046192	-1.565617	4.081254	0.000226	0.718960
-1.003450	-1.564165	4.091251	0.000218	0.718978
-0.956967	-1.421935	4.101248	0.000209	0.719276
-0.938191	-1.380752	4.111245	0.000205	0.719364
-0.861506	-1.270732	4.121242	0.000191	0.719608
-0.755344	-1.195019	4.131238	0.000171	0.719795
-0.534048	-1.174280	4.141235	0.000129	0.719914
-0.714318	-0.983069	4.151232	0.000163	0.720227
-0.631375	-0.904012	4.161229	0.000147	0.720413
-0.681524	-0.789962	4.171226	0.000156	0.720620
-0.387821	-0.708595	4.181222	0.000101	0.720883
-0.393823	-0.600588	4.191219	0.000102	0.721094
-0.071877	-0.549506	4.201216	0.000042	0.721308
-0.120198	-0.427384	4.211213	0.000051	0.721531
-0.226027	-0.278688	4.221210	0.000070	0.721787
-0.351207	-0.107413	4.231206	0.000093	0.722080
-0.333570	0.035195	4.241203	0.000090	0.722367
-0.294211	0.181398	4.251200	0.000082	0.722668
0.000000	0.305570	4.261197	0.000027	0.723015

0.282524	0.891793	4.266202	-0.000026	0.724263
0.442250	2.130222	4.271206	-0.000057	0.726741
0.790161	3.926559	4.276211	-0.000123	0.730360
0.894994	6.321928	4.281216	-0.000144	0.735034
1.188773	9.193315	4.286221	-0.000201	0.740656
1.296015	12.571040	4.291226	-0.000223	0.747135
1.706994	16.356101	4.296230	-0.000302	0.754426
2.201434	20.526817	4.301235	-0.000397	0.762393
2.431218	25.145511	4.306240	-0.000443	0.771015
2.723854	30.124916	4.311245	-0.000501	0.780219
3.115898	35.422785	4.316250	-0.000577	0.789918
3.581283	41.030856	4.321254	-0.000667	0.800073
3.912337	46.968117	4.326259	-0.000733	0.810636
4.224626	53.184140	4.331264	-0.000795	0.821538
4.739902	59.645542	4.336269	-0.000896	0.832776
5.200002	66.324719	4.341274	-0.000986	0.844214
5.671295	73.237859	4.346278	-0.001078	0.855890
6.315900	80.318438	4.351283	-0.001203	0.867733
6.438548	87.679973	4.356288	-0.001230	0.879720
7.150148	95.114558	4.361293	-0.001368	0.891827
9.437808	102.439223	4.366298	-0.001799	0.904033
10.252840	110.200759	4.371302	-0.001956	0.916352
11.056841	118.071639	4.376307	-0.002111	0.928671
11.865834	126.069931	4.381312	-0.002266	0.941022
12.965754	134.140327	4.386317	-0.002477	0.953395
13.573839	142.362108	4.391322	-0.002595	0.965705
14.487935	150.641687	4.396326	-0.002771	0.978021
15.505347	158.975789	4.401331	-0.002966	0.990287
16.542208	167.352672	4.406336	-0.003165	1.002467
17.536622	175.782911	4.411341	-0.003355	1.014565
18.446162	184.256305	4.416346	-0.003530	1.026560
19.362828	192.787834	4.421350	-0.003707	1.038496
20.160148	201.363126	4.426355	-0.003861	1.050327
21.104793	209.935027	4.431360	-0.004042	1.062056
22.303673	218.522813	4.436365	-0.004271	1.073734
23.130945	227.134458	4.441370	-0.004431	1.085234
23.753263	235.819306	4.446374	-0.004553	1.096662
24.646416	244.448101	4.451379	-0.004725	1.107959
25.305484	253.120646	4.456384	-0.004853	1.119147
26.296417	261.753832	4.461389	-0.005043	1.130245
27.146483	270.392226	4.466394	-0.005207	1.141211
28.293592	279.021096	4.471398	-0.005427	1.152124
29.158464	287.649853	4.476403	-0.005593	1.162874
29.590928	296.336893	4.481408	-0.005680	1.173507
30.464259	304.931908	4.486413	-0.005848	1.184024
31.699731	313.470533	4.491418	-0.006084	1.194453
32.430986	322.073742	4.496422	-0.006225	1.204768
32.978548	330.707656	4.501427	-0.006333	1.214993
33.675385	339.287453	4.506432	-0.006469	1.225100
34.628327	347.854331	4.511437	-0.006652	1.235159
34.971208	356.447256	4.516442	-0.006721	1.245048
35.674365	364.991434	4.521446	-0.006858	1.254872
36.884963	373.422755	4.526451	-0.007089	1.264590
37.236371	382.008596	4.531456	-0.007160	1.274243
38.034796	390.494518	4.536461	-0.007314	1.283797
38.417770	399.035994	4.541466	-0.007391	1.293264
39.116165	407.505690	4.546470	-0.007527	1.302641
39.535068	416.089891	4.551475	-0.007610	1.312024
40.168373	424.564267	4.556480	-0.007734	1.321262
40.503672	433.038503	4.561485	-0.007802	1.330381
40.881192	441.467292	4.566490	-0.007878	1.339397
41.570992	449.849358	4.571494	-0.008012	1.348359
41.994356	458.274504	4.576499	-0.008096	1.357260
42.287330	466.670767	4.581504	-0.008156	1.366050
43.627062	474.930039	4.586509	-0.008411	1.374822
44.264708	483.278645	4.591514	-0.008536	1.383510
44.332575	491.750923	4.596518	-0.008554	1.392173
44.770603	500.112418	4.601523	-0.008641	1.400733
45.520180	508.409671	4.606528	-0.008786	1.409227
46.184648	516.751146	4.611533	-0.008915	1.417701
46.487395	525.097556	4.616538	-0.008977	1.426069
47.270934	533.407144	4.621542	-0.009129	1.434430
47.740866	541.732059	4.626547	-0.009222	1.442707
47.942327	550.089417	4.631552	-0.009265	1.450925
48.348853	558.418573	4.636557	-0.009346	1.459102
48.634180	566.739331	4.641562	-0.009404	1.467206
49.292655	575.056477	4.646566	-0.009533	1.475321
49.868339	583.302865	4.651571	-0.009645	1.483310
50.341547	591.569893	4.656576	-0.009739	1.491260
51.072352	599.821678	4.661581	-0.009880	1.499193
51.710688	608.062865	4.666586	-0.010005	1.507060
52.304099	616.331616	4.671590	-0.010121	1.514905
53.025854	624.559431	4.676595	-0.010260	1.522690
53.497193	632.825646	4.681600	-0.010354	1.530433
54.206526	641.077135	4.686605	-0.010491	1.538159
54.497540	649.350265	4.691610	-0.010551	1.545804
55.075816	657.619665	4.696614	-0.010664	1.553451
55.182871	665.903190	4.701619	-0.010689	1.561003
55.772958	674.102746	4.706624	-0.010805	1.568513
56.420471	682.325816	4.711629	-0.010931	1.576017
56.893293	690.541310	4.716634	-0.011024	1.583453
57.526198	698.755922	4.721638	-0.011148	1.590877
57.829495	707.021777	4.726643	-0.011209	1.598264
58.158075	715.231117	4.731648	-0.011276	1.605571
58.983882	723.422804	4.736653	-0.011435	1.612899
59.454312	731.636046	4.741658	-0.011528	1.620162
59.971033	739.843291	4.746662	-0.011630	1.627395
60.484748	748.111938	4.751667	-0.011731	1.634647
60.862468	756.305912	4.756672	-0.011807	1.641785
61.179591	764.524219	4.761677	-0.011871	1.648904
61.392964	772.745484	4.766682	-0.011916	1.655981
61.844369	780.914373	4.771686	-0.012006	1.663015
62.341007	789.094096	4.776691	-0.012104	1.670035
62.786496	797.276445	4.781696	-0.012192	1.677020
63.277811	805.450183	4.786701	-0.012289	1.683975
63.596563	813.642683	4.791706	-0.012354	1.690895
64.069225	821.831181	4.796710	-0.012447	1.697803
64.409792	830.014643	4.801715	-0.012516	1.704661
64.880274	838.202904	4.806720	-0.012609	1.711512
65.435020	846.374904	4.811725	-0.012718	1.718334
65.589439	854.549863	4.816730	-0.012752	1.725079
65.840822	862.748116	4.821734	-0.012804	1.731830
66.180989	870.933902	4.826739	-0.012873	1.738555
66.618824	879.052055	4.831744	-0.012960	1.745212
66.996204	887.247422	4.836749	-0.013036	1.751898
67.726516	895.341742	4.841754	-0.013177	1.758521
68.529797	903.430100	4.846758	-0.013332	1.765124
68.877101	911.624029	4.851763	-0.013402	1.771729
69.126627	919.819225	4.856768	-0.013454	1.778299
69.405659	927.990461	4.861773	-0.013511	1.784829
69.845939	936.158450	4.866778	-0.013599	1.791353
70.264691	944.339597	4.871782	-0.013682	1.797860
70.627168	952.475991	4.876787	-0.013755	1.804302
71.079637	960.582245	4.881792	-0.013845	1.810708
71.488106	968.742879	4.886797	-0.013926	1.817128
72.009933	976.843984	4.891802	-0.014029	1.823493
72.426954	985.006776	4.896806	-0.014112	1.829871
72.725713	993.172510	4.901811	-0.014173	1.836215
73.185925	1001.276425	4.906816	-0.014264	1.842509
74.043978	1009.358162	4.911821	-0.014429	1.848810
74.268217	1017.536424	4.916826	-0.014476	1.855090
74.521930	1025.691963	4.921830	-0.014529	1.861334
75.183219	1033.789082	4.926835	-0.014657	1.867561
75.454177	1041.967137	4.931840	-0.014713	1.873782
75.799947	1050.114425	4.936845	-0.014783	1.879969
76.396116	1058.188455	4.941850	-0.014899	1.886108
76.668663	1066.357876	4.946854	-0.014955	1.892262
76.774747	1074.524984	4.951859	-0.014980	1.898376
77.072800	1082.635940	4.956864	-0.015041	1.904450
77.672060	1090.754712	4.961869	-0.015158	1.910543
77.903674	1098.897364	4.966874	-0.015207	1.916594
78.278165	1107.010943	4.971878	-0.015282	1.922621
78.609030	1115.131597	4.976883	-0.015349	1.928628
78.952758	1123.263367	4.981888	-0.015418	1.934627
79.393934	1131.370118	4.986893	-0.015506	1.940599
79.747444	1139.471187	4.991898	-0.015577	1.946539
80.288772	1147.624090	4.996902	-0.015683	1.952519
80.726516	1155.719508	5.001907	-0.015770	1.958428
81.080494	1163.802905	5.006912	-0.015841	1.964301
81.641355	1171.893419	5.011917	-0.015951	1.970184
81.803110	1180.036268	5.016922	-0.015987	1.976044
81.981521	1188.168191	5.021926	-0.016025	1.981880
82.301709	1196.270316	5.026931	-0.016090	1.987693
82.826754	1204.371103	5.031936	-0.016193	1.993510
83.371937	1212.461060	5.036941	-0.016300	1.999304
83.492537	1220.573241	5.041946	-0.016328	2.005053
84.026024	1228.662874	5.046950	-0.016433	2.010812
84.350554	1236.798777	5.051955	-0.016499	2.016565
84.713991	1244.893150	5.056960	-0.016572	2.022277
85.233183	1252.985561	5.061965	-0.016674	2.027987
85.414775	1261.136503	5.066970	-0.016713	2.033688
85.701215	1269.240217	5.071974	-0.016772	2.039350
86.078962	1277.315884	5.076979	-0.016847	2.044986
86.478507	1285.402368	5.081984	-0.016927	2.050617
86.814352	1293.514836	5.086989	-0.016995	2.056243
87.155894	1301.594183	5.091994	-0.017064	2.061832
87.649341	1309.684305	5.096998	-0.017161	2.067428
87.742536	1317.845672	5.102003	-0.017184	2.073017
87.688088	1325.968569	5.107008	-0.017179	2.078551
88.283922	1334.012674	5.112013	-0.017295	2.084081
88.660801	1342.098862	5.117018	-0.017371	2.089603
89.018495	1350.215076	5.122022	-0.017443	2.095128
89.339978	1358.299177	5.127027	-0.017508	2.100614
89.870048	1366.352718	5.132032	-0.017612	2.106085
90.310542	1374.497138	5.137037	-0.017699	2.111594
90.647968	1382.612657	5.142042	-0.017768	2.117060
91.220248	1390.660868	5.147046	-0.017880	2.122489
91.385352	1398.754832	5.152051	-0.017916	2.127895
91.628385	1406.862816	5.157056	-0.017966	2.133304
92.268042	1414.912831	5.162061	-0.018091	2.138699
92.781063	1422.956859	5.167066	-0.018192	2.144064
93.311144	1431.033463	5.172070	-0.018296	2.149439
93.481481	1439.187247	5.177075	-0.018333	2.154817
93.953424	1447.221610	5.182080	-0.018426	2.160132
94.242110	1455.332770	5.187085	-0.018485	2.165466
94.482569	1463.426001	5.192090	-0.018535	2.170771
94.650142	1471.546205	5.197094	-0.018572	2.176075
95.112721	1479.604386	5.202099	-0.018663	2.181351
95.371586	1487.687861	5.207104	-0.018717	2.186613
95.992388	1495.772766	5.212109	-0.018838	2.191896
96.384780	1503.854130	5.217114	-0.018916	2.197143
96.577956	1511.949654	5.222118	-0.018958	2.202369
96.923736	1520.011926	5.227123	-0.019027	2.207575
97.057793	1528.121038	5.232128	-0.019058	2.212779
97.342940	1536.221799	5.237133	-0.019116	2.217979
97.437053	1544.300377	5.242138	-0.019139	2.223136
97.840531	1552.365583	5.247142	-0.019219	2.228300
98.171524	1560.468305	5.252147	-0.019286	2.233469
98.616067	1568.496425	5.257152	-0.019374	2.238589
98.989202	1576.561123	5.262157	-0.019449	2.243714
99.347119	1584.636238	5.267162	-0.019521	2.248832
99.854875	1592.721393	5.272166	-0.019621	2.253958
100.245665	1600.783236	5.277171	-0.019699	2.259048
100.476043	1608.852296	5.282176	-0.019748	2.264116
101.015801	1616.941140	5.287181	-0.019853	2.269212
101.206379	1625.114597	5.292186	-0.019894	2.274320
101.571779	1633.143661	5.297190	-0.019968	2.279341
102.066323	1641.173168	5.302195	-0.020065	2.284362
102.216824	1649.251084	5.307200	-0.020098	2.289373
102.516627	1657.361754	5.312205	-0.020160	2.294405
102.884599	1665.398915	5.317210	-0.020233	2.299388
103.268416	1673.462030	5.322214	-0.020310	2.304376
103.502999	1681.548010	5.327219	-0.020359	2.309355
103.838609	1689.628378	5.332224	-0.020427	2.314328
104.422148	1697.648819	5.337229	-0.020541	2.319275
104.669462	1705.712817	5.342234	-0.020592	2.324210
104.790323	1713.817747	5.347238	-0.020620	2.329148
105.157931	1721.904940	5.352243	-0.020694	2.334086
105.399141	1729.964973	5.357248	-0.020744	2.338986
105.771975	1738.025825	5.362253	-0.020819	2.343887
106.271044	1746.064988	5.367258	-0.020917	2.348776
106.725303	1754.161315	5.372262	-0.021007	2.353684
107.063215	1762.227821	5.377267	-0.021076	2.358555
107.333812	1770.265797	5.382272	-0.021131	2.363393
107.671890	1778.339072	5.387277	-0.021200	2.368248
107.850483	1786.422528	5.392282	-0.021238	2.373086
108.229840	1794.487324	5.397286	-0.021314	2.377920
108.548870	1802.559247	5.402291	-0.021379	2.382742
108.670180	1810.633318	5.407296	-0.021407	2.387541
108.942938	1818.727551	5.412301	-0.021463	2.392354
109.392016	1826.760310	5.417306	-0.021552	2.397134
109.836841	1834.803351	5.422310	-0.021640	2.401911
110.244959	1842.865723	5.427315	-0.021721	2.406686
110.545679	1850.933080	5.432320	-0.021783	2.411447
111.159179	1858.989853	5.437325	-0.021902	2.416216
111.521301	1867.029392	5.442330	-0.021975	2.420946
111.774178	1875.105744	5.447334	-0.022028	2.425680
112.012735	1883.220320	5.452339	-0.022077	2.430426
112.206202	1891.354169	5.457344	-0.022119	2.435170
112.491651	1899.376155	5.462349	-0.022177	2.439847
112.857689	1907.396952	5.467354	-0.022251	2.444521
113.198619	1915.446906	5.472358	-0.022320	2.449200
113.444645	1923.530855	5.477363	-0.022371	2.453883
113.622009	1931.587560	5.482368	-0.022409	2.458536
114.097124	1939.627081	5.487373	-0.022503	2.463193
114.512004	1947.671726	5.492378	-0.022585	2.467839
114.957880	1955.738149	5.497382	-0.022674	2.472491
115.158784	1963.828070	5.502387	-0.022717	2.477129
115.507163	1971.849543	5.507392	-0.022787	2.481731
115.853047	1979.928716	5.512397	-0.022856	2.486357
116.198108	1987.962516	5.517402	-0.022926	2.490948
116.664546	1996.033442	5.522406	-0.023018	2.495561
116.960473	2004.100730	5.527411	-0.023079	2.500150
117.189902	2012.128285	5.532416	-0.023127	2.504704
117.603348	2020.197379	5.537421	-0.023209	2.509286
117.975465	2028.289289	5.542426	-0.023284	2.513870
117.992922	2036.358502	5.547430	-0.023292	2.518406
118.255587	2044.407882	5.552435	-0.023347	2.522942
118.777528	2052.399775	5.557440	-0.023449	2.527455
119.052457	2060.497011	5.562445	-0.023506	2.532001
119.366127	2068.547219	5.567450	-0.023569	2.536516
119.747553	2076.587661	5.572454	-0.023646	2.541022
120.341096	2084.601669	5.577459	-0.023762	2.545520
120.376751	2092.692434	5.582464	-0.023774	2.550014
120.930234	2100.763329	5.587469	-0.023882	2.554525
120.990291	2108.821023	5.592474	-0.023898	2.558986
121.304195	2116.852906	5.597478	-0.023962	2.563442
121.803526	2124.897744	5.602483	-0.024061	2.567911
121.925020	2132.981103	5.607488	-0.024088	2.572367
122.408101	2141.035192	5.612493	-0.024184	2.576824
122.693366	2149.083288	5.617498	-0.024242	2.581257
122.878100	2157.141132	5.622502	-0.024282	2.585680
123.368746	2165.193286	5.627507	-0.024379	2.590113
123.345671	2173.473095	5.632512	-0.024380	2.594628
124.030495	2181.421569	5.637517	-0.024513	2.599003
124.415613	2189.391784	5.642522	-0.024590	2.603362
124.527076	2197.425671	5.647526	-0.024616	2.607729
124.914877	2205.482703	5.652531	-0.024693	2.612121
125.148513	2213.506167	5.657536	-0.024742	2.616476
125.486066	2221.562724	5.662541	-0.024810	2.620849
125.555276	2229.617629	5.667546	-0.024828	2.625196
125.790287	2237.660013	5.672550	-0.024878	2.629539
126.392690	2245.706173	5.677555	-0.024995	2.633902
126.622333	2253.732554	5.682560	-0.025043	2.638223
126.920251	2261.788672	5.687565	-0.025104	2.642556
127.231372	2269.829702	5.692570	-0.025167	2.646876
127.572499	2277.868397	5.697574	-0.025236	2.651188
127.971752	2285.939401	5.702579	-0.025316	2.655515
128.303450	2293.958621	5.707584	-0.025383	2.659803
128.868070	2302.006218	5.712589	-0.025493	2.664114
128.896248	2310.088663	5.717594	-0.025504	2.668402
129.509947	2318.137420	5.722598	-0.025623	2.672702
129.912295	2326.210881	5.727603	-0.025704	2.676995
130.317459	2334.206026	5.732608	-0.025784	2.681240
130.717241	2342.234306	5.737613	-0.025864	2.685495
130.808677	2350.297813	5.742618	-0.025887	2.689743
131.071301	2358.373791	5.747622	-0.025941	2.694001
131.362965	2366.431222	5.752627	-0.026000	2.698244
131.464887	2374.451425	5.757632	-0.026025	2.702450
131.977719	2382.497234	5.762637	-0.026126	2.706688
132.115721	2390.564771	5.767642	-0.026157	2.710907
132.394297	2398.637810	5.772646	-0.026214	2.715131
132.525254	2406.682298	5.777651	-0.026244	2.719324
132.671156	2414.689395	5.782656	-0.026276	2.723493
133.224091	2422.733489	5.787661	-0.026384	2.727699
133.231044	2430.824777	5.792666	-0.026391	2.731890
133.535709	2438.887890	5.797670	-0.026453	2.736078
133.944850	2446.891909	5.802675	-0.026534	2.740235
134.156645	2454.920655	5.807680	-0.026579	2.744386
134.558053	2462.974605	5.812685	-0.026659	2.748556
134.648783	2471.101196	5.817690	-0.026682	2.752738
135.006548	2479.150467	5.822694	-0.026754	2.756890
135.574324	2487.127151	5.827699	-0.026865	2.761011
135.682191	2495.140474	5.832704	-0.026890	2.765117
136.164315	2503.175970	5.837709	-0.026985	2.769251
136.439236	2511.238069	5.842714	-0.027042	2.773379
136.681004	2519.262213	5.847718	-0.027092	2.777480
137.179221	2527.295650	5.852723	-0.027190	2.781595
137.465813	2535.312863	5.857728	-0.027249	2.785683
137.747719	2543.399868	5.862733	-0.027307	2.789800
137.933820	2551.486594	5.867738	-0.027347	2.793905
138.236449	2559.502686	5.872742	-0.027408	2.797975
138.982862	2567.496925	5.877747	-0.027552	2.802054
139.148431	2575.536450	5.882752	-0.027589	2.806116
139.545569	2583.594085	5.887757	-0.027668	2.810195
139.871124	2591.658171	5.892762	-0.027734	2.814267
140.097511	2599.716816	5.897766	-0.027781	2.818324
140.295409	2607.767390	5.902771	-0.027824	2.822370
140.508179	2615.794227	5.907776	-0.027868	2.826399
140.839842	2623.849773	5.912781	-0.027936	2.830443
140.939988	2631.950804	5.917786	-0.027960	2.834491
141.402441	2639.955368	5.922790	-0.028051	2.838505
141.678332	2647.990732	5.927795	-0.028108	2.842519
141.662745	2656.013909	5.932800	-0.028110	2.846505
141.980060	2664.051763	5.937805	-0.028174	2.850510
142.239233	2672.114581	5.942810	-0.028228	2.854520
142.606297	2680.123103	5.947814	-0.028302	2.858502
142.783326	2688.159237	5.952819	-0.028340	2.862483
142.973999	2696.208302	5.957824	-0.028381	2.866465
143.609128	2704.215878	5.962829	-0.028504	2.870445
143.809121	2712.285327	5.967834	-0.028547	2.874426
143.795676	2720.340229	5.972838	-0.028550	2.878383
144.196884	2728.365258	5.977843	-0.028630	2.882342
144.368355	2736.417454	5.982848	-0.028667	2.886297
144.445015	2744.469578	5.987853	-0.028687	2.890241
144.784812	2752.513913	5.992858	-0.028755	2.894190
144.887739	2760.557772	5.997862	-0.028780	2.898120
145.083704	2768.606863	6.002867	-0.028822	2.902053
145.242112	2776.630025	6.007872	-0.028856	2.905966
145.557028	2784.668786	6.012877	-0.028920	2.909889
145.607752	2792.806723	6.017882	-0.028935	2.913842
145.963444	2800.789627	6.022886	-0.029007	2.917729
146.420920	2808.805193	6.027891	-0.029097	2.921633
146.465932	2816.812661	6.032896	-0.029111	2.925506
146.819157	2824.834160	6.037901	-0.029182	2.929397
146.823472	2832.927060	6.042906	-0.029188	2.933298
147.321805	2840.916243	6.047910	-0.029286	2.937170
147.653042	2848.966147	6.052915	-0.029353	2.941058
147.854364	2856.947864	6.057920	-0.029396	2.944901
148.265187	2865.002903	6.062925	-0.029478	2.948785
148.568790	2873.043785	6.067930	-0.029540	2.952651
148.791527	2881.093603	6.072934	-0.029587	2.956512
149.078228	2889.124327	6.077939	-0.029645	2.960363
149.289811	2897.146191	6.082944	-0.029690	2.964200
149.621337	2905.192001	6.087949	-0.029757	2.968050
150.055272	2913.238188	6.092954	-0.029843	2.971900
150.163679	2921.310596	6.097958	-0.029869	2.975741
150.402207	2929.328336	6.102963	-0.029918	2.979557
150.544103	2937.357500	6.107968	-0.029950	2.983369
150.801854	2945.411166	6.112973	-0.030003	2.987194
150.836267	2953.463845	6.117978	-0.030015	2.991002
150.988882	2961.536859	6.122982	-0.030049	2.994821
151.310142	2969.544224	6.127987	-0.030114	2.998613
151.624156	2977.526174	6.132992	-0.030178	3.002387
151.772796	2985.589468	6.137997	-0.030211	3.006186
152.037937	2993.604976	6.143002	-0.030266	3.009964
152.114452	3001.672364	6.148006	-0.030285	3.013753
152.542052	3009.702042	6.153011	-0.030370	3.017535
152.630513	3017.743241	6.158016	-0.030392	3.021302
152.806813	3025.759344	6.163021	-0.030430	3.025057
153.151833	3033.786101	6.168026	-0.030500	3.028821
153.267676	3041.856104	6.173030	-0.030527	3.032588
153.646602	3049.911077	6.178035	-0.030602	3.036357
153.905270	3057.878474	6.183040	-0.030656	3.040074
154.254918	3065.930490	6.188045	-0.030726	3.043831
154.245783	3073.958740	6.193050	-0.030730	3.047554
154.508490	3081.995945	6.198054	-0.030784	3.051290
154.731210	3090.069511	6.203059	-0.030831	3.055037
154.997826	3098.079010	6.208064	-0.030886	3.058751
155.277174	3106.114690	6.213069	-0.030943	3.062473
155.423840	3114.158197	6.218074	-0.030976	3.066188
155.749735	3122.151304	6.223078	-0.031042	3.069884
156.180646	3130.267890	6.228083	-0.031127	3.073637
156.248055	3138.309616	6.233088	-0.031145	3.077334
156.736393	3146.298869	6.238093	-0.031242	3.081022
156.950195	3154.281949	6.243098	-0.031287	3.084690
157.190346	3162.330017	6.248102	-0.031337	3.088385
157.566207	3170.370150	6.253107	-0.031412	3.092078
157.794506	3178.410226	6.258112	-0.031460	3.095759
158.275587	3186.425855	6.263117	-0.031555	3.099437
158.394626	3194.469502	6.268122	-0.031582	3.103106
158.585536	3202.503231	6.273126	-0.031623	3.106769
159.018363	3210.543848	6.278131	-0.031709	3.110443
159.191491	3218.594458	6.283136	-0.031747	3.114105
159.400369	3226.636635	6.288141	-0.031791	3.117760
159.384660	3234.668440	6.293146	-0.031793	3.121396
159.634289	3242.669669	6.298150	-0.031845	3.125026
160.083771	3250.686281	6.303155	-0.031934	3.128668
160.396014	3258.721082	6.308160	-0.031997	3.132307
160.710721	3266.789411	6.313165	-0.032061	3.135957
160.976737	3274.790876	6.318170	-0.032116	3.139571
161.065582	3282.846066	6.323174	-0.032138	3.143197
161.489460	3290.872453	6.328179	-0.032222	3.146820
161.724700	3298.901558	6.333184	-0.032271	3.150432
162.145683	3306.984055	6.338189	-0.032355	3.154072
162.324866	3315.003869	6.343194	-0.032394	3.157669
162.659958	3322.981547	6.348198	-0.032462	3.161250
162.937737	3330.997749	6.353203	-0.032519	3.164842
163.142203	3339.039354	6.358208	-0.032562	3.168437
163.432294	3347.100923	6.363213	-0.032621	3.172041
163.518683	3355.150597	6.368218	-0.032643	3.175627
163.536489	3363.183645	6.373222	-0.032651	3.179199
163.831012	3371.214141	6.378227	-0.032712	3.182777
164.201596	3379.231099	6.383232	-0.032786	3.186348
164.290017	3387.284028	6.388237	-0.032808	3.189920
164.605898	3395.327310	6.393242	-0.032872	3.193492
164.715351	3403.355461	6.398246	-0.032898	3.197045
165.159960	3411.379385	6.403251	-0.032986	3.200607
165.471107	3419.357042	6.408256	-0.033049	3.204138
165.828248	3427.397485	6.413261	-0.033121	3.207695
166.005061	3435.458263	6.418266	-0.033159	3.211249
165.906702	3443.506906	6.423270	-0.033146	3.214783
166.149981	3451.526068	6.428275	-0.033197	3.218314
166.396394	3459.555297	6.433280	-0.033248	3.221846
166.548319	3467.582285	6.438285	-0.033281	3.225368
166.653447	3475.614621	6.443290	-0.033306	3.228888
166.864388	3483.673853	6.448294	-0.033351	3.232419
167.259864	3491.738559	6.453299	-0.033430	3.235957
167.388012	3499.702297	6.458304	-0.033459	3.239436
167.634455	3507.730459	6.463309	-0.033510	3.242944
167.986978	3515.731869	6.468314	-0.033581	3.246440
167.944068	3523.761776	6.473318	-0.033578	3.249930
168.349749	3531.807494	6.478323	-0.033659	3.253440
168.666563	3539.827731	6.483328	-0.033724	3.256932
168.799638	3547.861924	6.488333	-0.033754	3.260419
168.902295	3555.877968	6.493338	-0.033778	3.263893
168.978298	3563.934641	6.498342	-0.033798	3.267380
169.295760	3571.971629	6.503347	-0.033862	3.270864
169.319293	3580.019251	6.508352	-0.033872	3.274338
169.705716	3588.031904	6.513357	-0.033949	3.277807
169.941329	3596.066785	6.518362	-0.033998	3.281276
170.305750	3604.010877	6.523366	-0.034071	3.284707
170.393821	3612.107394	6.528371	-0.034093	3.288189
170.539607	3620.140442	6.533376	-0.034126	3.291643
171.011753	3628.171163	6.538381	-0.034219	3.295104
171.114069	3636.206224	6.543386	-0.034243	3.298549
171.277495	3644.218045	6.548390	-0.034279	3.301984
171.769962	3652.232580	6.553395	-0.034376	3.305428
171.805547	3660.279941	6.558400	-0.034388	3.308865
171.929309	3668.344043	6.563405	-0.034416	3.312309
172.252735	3676.376340	6.568410	-0.034482	3.315744
172.541910	3684.359219	6.573414	-0.034541	3.319152
172.678618	3692.403455	6.578419	-0.034572	3.322578
172.771504	3700.392969	6.583424	-0.034594	3.325975
173.309173	3708.423386	6.588429	-0.034700	3.329402
173.766704	3716.438356	6.593434	-0.034790	3.332817
174.023193	3724.493213	6.598438	-0.034843	3.336237
174.214792	3732.509648	6.603443	-0.034884	3.339635
174.390964	3740.540113	6.608448	-0.034922	3.343035
174.563737	3748.590977	6.613453	-0.034960	3.346439
174.673901	3756.614028	6.618458	-0.034986	3.349827
175.071677	3764.642861	6.623462	-0.035065	3.353224
175.382433	3772.713450	6.628467	-0.035128	3.356631
175.274425	3780.719638	6.633472	-0.035114	3.359993
175.692308	3788.733675	6.638477	-0.035197	3.363374
175.938718	3796.767562	6.643482	-0.035248	3.366754
176.080841	3804.780474	6.648486	-0.035280	3.370117
176.560919	3812.850489	6.653491	-0.035374	3.373513
176.837115	3820.851228	6.658496	-0.035431	3.376870
176.920367	3828.880031	6.663501	-0.035452	3.380228
177.278812	3836.892276	6.668506	-0.035524	3.383585
177.451241	3844.928979	6.673510	-0.035561	3.386943
177.599974	3852.973476	6.678515	-0.035594	3.390300
177.615619	3861.081391	6.683520	-0.035603	3.393675
177.964052	3869.117145	6.688525	-0.035673	3.397028
178.204362	3877.048914	6.693530	-0.035723	3.400331
178.427364	3885.041882	6.698534	-0.035770	3.403656
178.674548	3893.094277	6.703539	-0.035821	3.407003
178.945726	3901.072795	6.708544	-0.035877	3.410317
179.359736	3909.115418	6.713549	-0.035959	3.413658
179.532991	3917.170742	6.718554	-0.035997	3.416994
179.735121	3925.157538	6.723558	-0.036040	3.420299
180.096705	3933.182315	6.728563	-0.036112	3.423622
180.210218	3941.244342	6.733568	-0.036139	3.426948
180.729045	3949.242680	6.738573	-0.036241	3.430259
180.798834	3957.315725	6.743578	-0.036259	3.433582
180.887779	3965.360881	6.748582	-0.036281	3.436891
181.081667	3973.348321	6.753587	-0.036322	3.440176
181.437119	3981.351073	6.758592	-0.036394	3.443470
181.526223	3989.433328	6.763597	-0.036416	3.446785
181.715054	3997.462024	6.768602	-0.036456	3.450078
181.956014	4005.481343	6.773606	-0.036507	3.453365
182.189942	4013.548737	6.778611	-0.036555	3.456669
182.297684	4021.519201	6.783616	-0.036581	3.459926
182.630586	4029.549867	6.788621	-0.036648	3.463211
182.798479	4037.602892	6.793626	-0.036685	3.466498
182.884071	4045.621783	6.798630	-0.036706	3.469764
183.182170	4053.674590	6.803635	-0.036767	3.473048
183.419071	4061.704596	6.808640	-0.036816	3.476318
183.877011	4069.684974	6.813645	-0.036907	3.479571
183.970259	4077.698410	6.818650	-0.036929	3.482823
184.332421	4085.677642	6.823654	-0.037002	3.486067
184.612132	4093.711014	6.828659	-0.037060	3.489327
184.749687	4101.763815	6.833664	-0.037091	3.492588
184.933584	4109.798983	6.838669	-0.037130	3.495839
185.125219	4117.820232	6.843674	-0.037171	3.499082
185.145941	4125.851306	6.848678	-0.037180	3.502321
185.380217	4133.860283	6.853683	-0.037229	3.505554
185.542869	4141.876036	6.858688	-0.037265	3.508785
185.778255	4149.953530	6.863693	-0.037314	3.512040
185.931116	4157.971044	6.868698	-0.037348	3.515266
186.244556	4165.978370	6.873702	-0.037411	3.518489
186.549777	4174.024973	6.878707	-0.037474	3.521725
186.551316	4182.001458	6.883712	-0.037479	3.524920
186.787434	4190.060402	6.888717	-0.037528	3.528152
187.101754	4198.089739	6.893722	-0.037592	3.531372
187.430218	4206.112206	6.898726	-0.037659	3.534587
187.661583	4214.178341	6.903731	-0.037707	3.537813
187.797062	4222.176850	6.908736	-0.037738	3.541007
188.099655	4230.207083	6.913741	-0.037799	3.544215
188.129247	4238.237499	6.918746	-0.037810	3.547412
188.306749	4246.235977	6.923750	-0.037849	3.550598
188.593915	4254.388516	6.928755	-0.037907	3.553846
188.792785	4262.385966	6.933760	-0.037950	3.557026
188.871630	4270.345128	6.938765	-0.037970	3.560185
189.153876	4278.365112	6.943770	-0.038028	3.563371
189.184809	4286.364182	6.948774	-0.038039	3.566539
189.283611	4294.374137	6.953779	-0.038062	3.569710
189.654275	4302.420557	6.958784	-0.038137	3.572900
190.027067	4310.454415	6.963789	-0.038211	3.576083
190.058514	4318.429959	6.968794	-0.038223	3.579230
190.376520	4326.446617	6.973798	-0.038287	3.582398
190.733714	4334.475646	6.978803	-0.038359	3.585570
190.996189	4342.500469	6.983808	-0.038413	3.588734
191.169900	4350.538040	6.988813	-0.038451	3.591898
191.571236	4358.571365	6.993818	-0.038531	3.595064
191.807015	4366.555247	6.998822	-0.038580	3.598204
191.910503	4374.625686	7.003827	-0.038605	3.601370
192.132684	4382.602407	7.008832	-0.038651	3.604501
192.625297	4390.627804	7.013837	-0.038748	3.607655
192.534380	4398.675829	7.018842	-0.038737	3.610799
192.858479	4406.699404	7.023846	-0.038802	3.613942
193.222813	4414.750519	7.028851	-0.038876	3.617095
193.400696	4422.756122	7.033856	-0.038914	3.620221
193.682038	4430.768773	7.038861	-0.038972	3.623351
193.997119	4438.808618	7.043866	-0.039036	3.626489
194.070665	4446.799962	7.048870	-0.039055	3.629599
194.111778	4454.914562	7.053875	-0.039068	3.632754
194.246992	4462.936473	7.058880	-0.039098	3.635872
194.513201	4470.942695	7.063885	-0.039153	3.638985
194.721961	4478.943700	7.068890	-0.039197	3.642091
194.785177	4486.948629	7.073894	-0.039214	3.645193
195.400767	4494.947181	7.078899	-0.039334	3.648304
195.512763	4503.004661	7.083904	-0.039360	3.651422
195.630485	4511.061422	7.088909	-0.039388	3.654537
196.046155	4519.086482	7.093914	-0.039470	3.657645
196.072074	4527.073399	7.098918	-0.039481	3.660726
196.248916	4535.125885	7.103923	-0.039519	3.663833
196.279513	4543.142298	7.108928	-0.039530	3.666920
196.695202	4551.161835	7.113933	-0.039612	3.670015
196.766276	4559.211970	7.118938	-0.039631	3.673110
197.039635	4567.222228	7.123942	-0.039687	3.676193
197.197104	4575.214404	7.128947	-0.039722	3.679263
197.402771	4583.246021	7.133952	-0.039765	3.682347
197.604023	4591.236646	7.138957	-0.039808	3.685412
197.707767	4599.282823	7.143962	-0.039833	3.688494
197.907809	4607.293579	7.148966	-0.039875	3.691562
198.281024	4615.344830	7.153971	-0.039950	3.694647
198.378731	4623.352884	7.158976	-0.039974	3.697707
198.591572	4631.370845	7.163981	-0.040019	3.700770
198.768417	4639.377376	7.168986	-0.040057	3.703825
199.057933	4647.423580	7.173990	-0.040116	3.706896
199.415352	4655.429567	7.178995	-0.040188	3.709951
199.523626	4663.491046	7.184000	-0.040214	3.713018
199.625960	4671.595805	7.189005	-0.040238	3.716099
199.927821	4679.550694	7.194010	-0.040299	3.719125
200.108686	4687.531366	7.199014	-0.040338	3.722155
200.430384	4695.514720	7.204019	-0.040404	3.725188
200.398206	4703.543411	7.209024	-0.040403	3.728226
200.680709	4711.591185	7.214029	-0.040461	3.731277
200.991249	4719.629883	7.219034	-0.040524	3.734323
200.845782	4727.672176	7.224038	-0.040502	3.737356
201.106237	4735.694166	7.229043	-0.040556	3.740389
201.402687	4743.671692	7.234048	-0.040617	3.743404
201.337722	4751.722786	7.239053	-0.040610	3.746435
201.703228	4759.742372	7.244058	-0.040683	3.749462
201.879022	4767.761102	7.249062	-0.040721	3.752482
202.155446	4775.790219	7.254067	-0.040778	3.755506
202.447438	4783.810020	7.259072	-0.040838	3.758524
202.645372	4791.842929	7.264077	-0.040880	3.761542
202.961687	4799.803594	7.269082	-0.040944	3.764534
202.928430	4807.875137	7.274086	-0.040943	3.767557
203.243958	4815.869665	7.279091	-0.041007	3.770556
203.433619	4823.930839	7.284096	-0.041048	3.773575
203.810104	4831.979913	7.289101	-0.041123	3.776591
203.936749	4839.950044	7.294106	-0.041152	3.779570
204.247846	4848.009376	7.299110	-0.041215	3.782584
204.587385	4855.996524	7.304115	-0.041284	3.785568
204.502426	4864.052805	7.309120	-0.041273	3.788567
204.893273	4872.066599	7.314125	-0.041352	3.791559
205.222441	4880.127453	7.319130	-0.041418	3.794564
205.386297	4888.113690	7.324134	-0.041454	3.797535
205.751049	4896.124056	7.329139	-0.041527	3.800517
205.931248	4904.130497	7.334144	-0.041566	3.803491
205.971960	4912.153849	7.339149	-0.041579	3.806467
206.132963	4920.184191	7.344154	-0.041614	3.809445
206.506882	4928.195219	7.349158	-0.041689	3.812418
206.962620	4936.235877	7.354163	-0.041779	3.815401
206.894784	4944.216421	7.359168	-0.041772	3.818349
207.398441	4952.245199	7.364173	-0.041871	3.821324
207.562833	4960.250500	7.369178	-0.041907	3.824281
207.598808	4968.283693	7.374182	-0.041919	3.827244
207.807835	4976.305813	7.379187	-0.041963	3.830203
208.152098	4984.350446	7.384192	-0.042033	3.833172
208.241359	4992.376594	7.389197	-0.042055	3.836126
208.386021	5000.360018	7.394202	-0.042087	3.839063
208.729855	5008.388803	7.399206	-0.042156	3.842019
209.149765	5016.373784	7.404211	-0.042240	3.844957
209.261134	5024.438193	7.409216	-0.042266	3.847917
209.410167	5032.475271	7.414221	-0.042299	3.850865
209.440423	5040.518219	7.419226	-0.042310	3.853810
209.615687	5048.553501	7.424230	-0.042348	3.856753
209.769964	5056.559401	7.429235	-0.042382	3.859683
210.143758	5064.580161	7.434240	-0.042457	3.862620
210.279044	5072.592607	7.439245	-0.042487	3.865547
210.292419	5080.690496	7.444250	-0.042495	3.868501
210.428896	5088.699763	7.449254	-0.042526	3.871422
210.775391	5096.914986	7.454259	-0.042596	3.874421
210.801811	5104.841225	7.459264	-0.042606	3.877305
210.957358	5112.761433	7.464269	-0.042640	3.880188
211.372461	5120.768541	7.469274	-0.042723	3.883105
211.361345	5128.745638	7.474278	-0.042726	3.886001
211.624433	5136.771229	7.479283	-0.042780	3.888918
211.947591	5144.812773	7.484288	-0.042846	3.891839
212.425659	5152.839568	7.489293	-0.042940	3.894756
212.196481	5160.864998	7.494298	-0.042903	3.897656
212.511893	5168.866659	7.499302	-0.042967	3.900556
213.019130	5176.868076	7.504307	-0.043066	3.903458
213.299505	5184.850031	7.509312	-0.043124	3.906346
213.483902	5192.895677	7.514317	-0.043164	3.909253
213.663680	5200.951096	7.519322	-0.043202	3.912161
213.775303	5208.943217	7.524326	-0.043229	3.915043
214.011933	5216.990531	7.529331	-0.043278	3.917944
214.338549	5224.964780	7.534336	-0.043344	3.920820
214.389277	5232.959613	7.539341	-0.043359	3.923695
214.910822	5241.004833	7.544346	-0.043461	3.926595
215.019249	5248.996570	7.549350	-0.043487	3.929466
215.337662	5257.061374	7.554355	-0.043551	3.932364
215.365259	5265.070703	7.559360	-0.043562	3.935236
215.565620	5273.106255	7.564365	-0.043604	3.938118
215.867311	5281.113204	7.569370	-0.043666	3.940989
215.983666	5289.070472	7.574374	-0.043693	3.943837
216.246967	5297.162789	7.579379	-0.043747	3.946734
216.300241	5305.178550	7.584384	-0.043762	3.949598
216.600724	5313.201482	7.589389	-0.043824	3.952467
216.679213	5321.266330	7.594394	-0.043844	3.955344
216.750663	5329.231386	7.599398	-0.043862	3.958184
217.179677	5337.238834	7.604403	-0.043947	3.961043
217.458135	5345.214569	7.609408	-0.044005	3.963886
217.474038	5353.278695	7.614413	-0.044013	3.966754
217.730792	5361.295268	7.619418	-0.044066	3.969606
217.760310	5369.316828	7.624422	-0.044077	3.972455
217.926755	5377.379213	7.629427	-0.044113	3.975319
218.101418	5385.376646	7.634432	-0.044151	3.978157
218.569560	5393.357622	7.639437	-0.044243	3.980993
218.757395	5401.379325	7.644442	-0.044284	3.983836
218.982059	5409.387520	7.649446	-0.044331	3.986673
219.044216	5417.447733	7.654451	-0.044348	3.989524
219.100439	5425.504288	7.659456	-0.044364	3.992371
219.278838	5433.534615	7.664461	-0.044402	3.995209
219.518766	5441.567991	7.669466	-0.044452	3.998047
219.506559	5449.557253	7.674470	-0.044455	4.000863
219.709264	5457.581653	7.679475	-0.044498	4.003693
220.002521	5465.588321	7.684480	-0.044558	4.006516
220.355951	5473.581265	7.689485	-0.044629	4.009334
220.575879	5481.655107	7.694490	-0.044675	4.012175
220.691194	5489.632631	7.699494	-0.044702	4.014979
220.891324	5497.696641	7.704499	-0.044745	4.017813
221.190669	5505.685602	7.709504	-0.044806	4.020620
221.047472	5513.733981	7.714509	-0.044785	4.023439
221.425682	5521.750565	7.719514	-0.044860	4.026253
221.595096	5529.750559	7.724518	-0.044897	4.029056
221.934556	5537.790089	7.729523	-0.044966	4.031874
221.899498	5545.908320	7.734528	-0.044964	4.034711
222.468805	5553.885375	7.739533	-0.045076	4.037506
222.674588	5561.831452	7.744538	-0.045119	4.040282
222.821467	5569.832983	7.749542	-0.045152	4.043076
223.176078	5577.847673	7.754547	-0.045223	4.045874
223.261004	5585.839694	7.759552	-0.045244	4.048660
223.328738	5593.893590	7.764557	-0.045262	4.051464
223.590338	5601.932650	7.769562	-0.045316	4.054264
223.938718	5609.938833	7.774566	-0.045387	4.057052
224.181999	5617.942324	7.779571	-0.045437	4.059836
224.302169	5625.947354	7.784576	-0.045465	4.062616
224.695345	5633.924531	7.789581	-0.045543	4.065389
224.786764	5641.985069	7.794586	-0.045566	4.068184
224.939766	5649.981149	7.799590	-0.045600	4.070956
225.189660	5658.056531	7.804595	-0.045651	4.073755
225.225929	5666.095375	7.809600	-0.045663	4.076537
225.468645	5674.065751	7.814605	-0.045714	4.079295
225.576836	5682.110120	7.819610	-0.045739	4.082076
225.803165	5690.024304	7.824614	-0.045787	4.084811
226.138563	5698.124389	7.829619	-0.045855	4.087610
226.111044	5706.094535	7.834624	-0.045855	4.090357
226.362784	5714.173666	7.839629	-0.045907	4.093144
226.720608	5722.213594	7.844634	-0.045979	4.095916
226.629646	5730.196085	7.849638	-0.045967	4.098662
227.020019	5738.240416	7.854643	-0.046045	4.101432
227.266670	5746.239338	7.859648	-0.046097	4.104184
227.376719	5754.254241	7.864653	-0.046122	4.106937
227.594071	5762.270634	7.869658	-0.046168	4.109690
227.759698	5770.319894	7.874662	-0.046204	4.112452
228.029465	5778.390909	7.879667	-0.046260	4.115221
228.037936	5786.393017	7.884672	-0.046267	4.117962
228.347388	5794.338536	7.889677	-0.046330	4.120684
228.728594	5802.367248	7.894682	-0.046406	4.123434
228.802919	5810.356652	7.899686	-0.046425	4.126166
229.008603	5818.428133	7.904691	-0.046469	4.128924
229.221874	5826.420649	7.909696	-0.046514	4.131655
229.194604	5834.499302	7.914701	-0.046514	4.134409
229.384893	5842.575774	7.919706	-0.046555	4.137164
229.678110	5850.496442	7.924710	-0.046615	4.139866
229.774483	5858.533780	7.929715	-0.046638	4.142602
229.967394	5866.527273	7.934720	-0.046679	4.145323
230.238049	5874.576753	7.939725	-0.046735	4.148063
230.437655	5882.618444	7.944730	-0.046777	4.150797
230.543996	5890.637382	7.949734	-0.046802	4.153520
230.693486	5898.671240	7.954739	-0.046836	4.156247
230.782749	5906.651644	7.959744	-0.046857	4.158953
230.972560	5914.662548	7.964749	-0.046898	4.161670
231.269999	5922.649413	7.969754	-0.046959	4.164377
231.587349	5930.696339	7.974758	-0.047023	4.167103
231.844011	5938.701688	7.979763	-0.047076	4.169813
231.858522	5946.729402	7.984768	-0.047084	4.172525
232.270668	5954.728349	7.989773	-0.047166	4.175231
232.443978	5962.782835	7.994778	-0.047204	4.177951
232.710301	5970.760065	7.999782	-0.047259	4.180644
232.869445	5978.812646	8.004787	-0.047294	4.183359
232.807237	5986.813464	8.009792	-0.047288	4.186053
233.145912	5994.815326	8.014797	-0.047356	4.188750
233.354141	6002.871082	8.019802	-0.047400	4.191462
233.481815	6010.940193	8.024806	-0.047429	4.194176
233.795400	6018.977321	8.029811	-0.047493	4.196879
233.998238	6026.904039	8.034816	-0.047536	4.199542
234.019214	6034.948397	8.039821	-0.047545	4.202241
234.253284	6042.911472	8.044826	-0.047594	4.204913
234.514407	6050.974919	8.049830	-0.047648	4.207617
234.720229	6058.977212	8.054835	-0.047692	4.210299
234.829125	6067.007135	8.059840	-0.047717	4.212987
235.186506	6074.986452	8.064845	-0.047789	4.215658
235.366888	6083.048988	8.069850	-0.047828	4.218355
235.349444	6090.999939	8.074854	-0.047830	4.221010
235.567975	6099.039002	8.079859	-0.047876	4.223695
235.705195	6107.052808	8.084864	-0.047907	4.226369
235.926473	6115.047845	8.089869	-0.047953	4.229036
236.260662	6123.126439	8.094874	-0.048021	4.231731
236.587887	6131.113897	8.099878	-0.048087	4.234393
236.648109	6139.195531	8.104883	-0.048104	4.237082
236.827218	6147.120347	8.109888	-0.048142	4.239719
236.954079	6155.189755	8.114893	-0.048171	4.242401
237.161884	6163.149294	8.119898	-0.048215	4.245046
237.298208	6171.194850	8.124902	-0.048246	4.247717
237.602235	6179.193061	8.129907	-0.048308	4.250373
237.827612	6187.244647	8.134912	-0.048355	4.253043
237.928318	6195.271651	8.139917	-0.048379	4.255703
237.957253	6203.317850	8.144922	-0.048390	4.258366
238.195735	6211.292913	8.149926	-0.048440	4.261007
238.512762	6219.349426	8.154931	-0.048504	4.263673
238.760968	6227.323066	8.159936	-0.048555	4.266309
238.959124	6235.382455	8.164941	-0.048598	4.268972
239.114070	6243.451829	8.169946	-0.048632	4.271636
239.268476	6251.480868	8.174950	-0.048666	4.274285
239.637129	6259.495485	8.179955	-0.048740	4.276930
239.629199	6267.430521	8.184960	-0.048744	4.279543
239.754712	6275.473450	8.189965	-0.048772	4.282191
240.288257	6283.443285	8.194970	-0.048877	4.284817
240.196036	6291.486304	8.199974	-0.048865	4.287461
240.355687	6299.483644	8.204979	-0.048900	4.290089
240.636056	6307.557330	8.209984	-0.048958	4.292742
240.888154	6315.549228	8.214989	-0.049010	4.295367
240.977322	6323.639386	8.219994	-0.049032	4.298021
240.920477	6331.574969	8.224998	-0.049027	4.300621
241.316811	6339.645265	8.230003	-0.049106	4.303267
241.577477	6347.629281	8.235008	-0.049160	4.305882
241.699144	6355.618486	8.240013	-0.049188	4.308497
242.096506	6363.649522	8.245018	-0.049267	4.311125
242.405210	6371.711459	8.250022	-0.049330	4.313761
242.381028	6379.723482	8.255027	-0.049330	4.316377
242.735252	6387.684414	8.260032	-0.049402	4.318978
242.945231	6395.696445	8.265037	-0.049446	4.321592
243.128095	6403.723573	8.270042	-0.049485	4.324209
243.210387	6411.734729	8.275046	-0.049506	4.326819
243.466368	6419.762532	8.280051	-0.049559	4.329434
243.470517	6427.816762	8.285056	-0.049565	4.332055
243.534060	6435.847782	8.290061	-0.049582	4.334666
243.776402	6443.850304	8.295066	-0.049633	4.337268
243.831761	6451.839326	8.300070	-0.049648	4.339863
244.034250	6459.858176	8.305075	-0.049691	4.342467
244.087644	6467.839573	8.310080	-0.049707	4.345056
244.492665	6475.868127	8.315085	-0.049787	4.347661
244.670883	6483.912737	8.320090	-0.049826	4.350268
244.818855	6491.968611	8.325094	-0.049859	4.352877
245.181801	6500.057227	8.330099	-0.049932	4.355496
245.517258	6508.027757	8.335104	-0.049999	4.358076
245.638292	6515.943289	8.340109	-0.050027	4.360635
245.787011	6524.017731	8.345114	-0.050060	4.363243
245.872327	6531.965661	8.350118	-0.050081	4.365809
246.087795	6540.034112	8.355123	-0.050127	4.368413
246.332808	6548.021715	8.360128	-0.050178	4.370990
246.635943	6556.013133	8.365133	-0.050240	4.373566
246.960906	6564.077878	8.370138	-0.050305	4.376165
246.975508	6572.072253	8.375142	-0.050313	4.378738
247.240783	6580.094348	8.380147	-0.050368	4.381320
247.498907	6588.078658	8.385152	-0.050421	4.383888
247.634715	6596.114472	8.390157	-0.050452	4.386470
247.898151	6604.153029	8.395162	-0.050506	4.389052
248.144752	6612.181130	8.400166	-0.050558	4.391629
248.301820	6620.197930	8.405171	-0.050592	4.394201
248.359253	6628.275611	8.410176	-0.050608	4.396790
248.603928	6636.217741	8.415181	-0.050659	4.399335
248.948081	6644.248923	8.420186	-0.050728	4.401907
248.989962	6652.188915	8.425190	-0.050742	4.404448
249.094942	6660.267374	8.430195	-0.050766	4.407031
249.400222	6668.237279	8.435200	-0.050829	4.409579
249.439784	6676.300806	8.440205	-0.050841	4.412155
249.499453	6684.360957	8.445210	-0.050858	4.414728
249.931416	6692.349185	8.450214	-0.050943	4.417278
250.388217	6700.351666	8.455219	-0.051034	4.419831
250.228347	6708.418283	8.460224	-0.051009	4.422400
250.398036	6716.377256	8.465229	-0.051046	4.424935
250.801197	6724.450650	8.470234	-0.051127	4.427506
250.920184	6732.434398	8.475238	-0.051154	4.430046
251.209058	6740.517880	8.480243	-0.051213	4.432617
251.477540	6748.544503	8.485248	-0.051269	4.435168
251.657126	6756.542536	8.490253	-0.051307	4.437708
251.637990	6764.467930	8.495258	-0.051309	4.440222
251.720991	6772.523624	8.500262	-0.051330	4.442778
252.056939	6780.533725	8.505267	-0.051398	4.445318
251.994017	6788.611333	8.510272	-0.051391	4.447876
252.252960	6796.548852	8.515277	-0.051445	4.450390
252.497945	6804.656942	8.520282	-0.051496	4.452956
252.522693	6812.604347	8.525286	-0.051506	4.455469
252.629714	6820.675921	8.530291	-0.051531	4.458021
252.846637	6828.620498	8.535296	-0.051577	4.460531
253.092735	6836.642545	8.540301	-0.051628	4.463064
253.206063	6844.663681	8.545306	-0.051654	4.465595
253.290697	6852.671881	8.550310	-0.051675	4.468120
253.731652	6860.725753	8.555315	-0.051763	4.470660
253.759939	6868.792319	8.560320	-0.051773	4.473201
253.981953	6876.726742	8.565325	-0.051820	4.475699
254.115525	6884.817393	8.570330	-0.051850	4.478244
254.150971	6892.739779	8.575335	-0.051862	4.480735
254.518234	6900.755096	8.580339	-0.051936	4.483255
254.756998	6908.769224	8.585344	-0.051985	4.485773
254.796734	6916.820477	8.590349	-0.051998	4.488300
255.014795	6924.814100	8.595354	-0.052044	4.490808
255.159111	6932.866665	8.600359	-0.052076	4.493333
255.527489	6940.870244	8.605363	-0.052150	4.495842
255.511532	6948.905319	8.610368	-0.052152	4.498359
255.586032	6956.852430	8.615373	-0.052172	4.500846
256.041803	6964.917010	8.620378	-0.052262	4.503370
256.212804	6972.890425	8.625383	-0.052299	4.505863
256.287832	6980.940948	8.630387	-0.052318	4.508379
256.330846	6988.969220	8.635392	-0.052332	4.510886
256.342935	6997.045206	8.640397	-0.052339	4.513407
256.770925	7005.083069	8.645402	-0.052424	4.515915
256.848896	7013.011511	8.650407	-0.052444	4.518387
257.112478	7021.008387	8.655411	-0.052498	4.520879
257.257331	7029.079653	8.660416	-0.052531	4.523393
257.524854	7037.013332	8.665421	-0.052586	4.525863
257.674351	7045.097646	8.670426	-0.052619	4.528378
257.761062	7053.036173	8.675431	-0.052640	4.530846
257.977119	7061.138234	8.680435	-0.052686	4.533364
258.364365	7069.140516	8.685440	-0.052763	4.535850
258.457427	7077.113457	8.690445	-0.052786	4.538325
258.614738	7085.150920	8.695450	-0.052820	4.540818
258.749823	7093.138571	8.700455	-0.052851	4.543295
259.140200	7101.189104	8.705459	-0.052929	4.545790
259.370050	7109.190367	8.710464	-0.052977	4.548268
259.655998	7117.196904	8.715469	-0.053036	4.550747
259.996024	7125.269326	8.720474	-0.053104	4.553245
260.039421	7133.292707	8.725479	-0.053118	4.555725
260.040578	7141.303429	8.730483	-0.053123	4.558201
260.373646	7149.283231	8.735488	-0.053190	4.560666
260.673004	7157.275667	8.740493	-0.053252	4.563133
260.974755	7165.280647	8.745498	-0.053313	4.565603
260.946584	7173.294846	8.750503	-0.053313	4.568074
261.220712	7181.340154	8.755507	-0.053369	4.570553
261.401868	7189.353608	8.760512	-0.053408	4.573022
261.558296	7197.366438	8.765517	-0.053443	4.575488
261.795943	7205.430242	8.770522	-0.053492	4.577969
262.001257	7213.375676	8.775527	-0.053536	4.580413
262.035978	7221.430263	8.780531	-0.053548	4.582888
262.089174	7229.378397	8.785536	-0.053563	4.585329
262.389983	7237.457807	8.790541	-0.053624	4.587810
262.755541	7245.511160	8.795546	-0.053698	4.590281
262.897581	7253.525254	8.800551	-0.053729	4.592739
263.061388	7261.563064	8.805555	-0.053765	4.595202
263.161973	7269.579760	8.810560	-0.053789	4.597658
263.386412	7277.532503	8.815565	-0.053836	4.600093
263.581486	7285.619144	8.820570	-0.053878	4.602567
263.740090	7293.503935	8.825575	-0.053913	4.604979
263.955666	7301.623871	8.830579	-0.053958	4.607461
263.854179	7309.589459	8.835584	-0.053945	4.609894
264.387721	7317.672614	8.840589	-0.054049	4.612362
264.645090	7325.655501	8.845594	-0.054103	4.614798
264.750079	7333.663941	8.850599	-0.054127	4.617241
264.965941	7341.642063	8.855603	-0.054173	4.619673
265.168401	7349.699271	8.860608	-0.054216	4.622128
265.206926	7357.625098	8.865613	-0.054228	4.624541
265.324573	7365.729713	8.870618	-0.054256	4.627008
265.550282	7373.731219	8.875623	-0.054303	4.629442
265.666619	7381.768547	8.880627	-0.054330	4.631886
265.830983	7389.826768	8.885632	-0.054366	4.634334
265.930543	7397.777032	8.890637	-0.054390	4.636749
266.085875	7405.833530	8.895642	-0.054424	4.639194
266.108554	7413.780628	8.900647	-0.054434	4.641605
266.565637	7421.814949	8.905651	-0.054524	4.644041
266.752681	7429.815461	8.910656	-0.054564	4.646466
266.714661	7437.866675	8.915661	-0.054562	4.648905
266.991404	7445.883315	8.920666	-0.054619	4.651331
267.241419	7453.886587	8.925671	-0.054671	4.653753
267.203264	7461.916457	8.930675	-0.054669	4.656181
267.300747	7469.921251	8.935680	-0.054693	4.658601
267.667754	7477.897579	8.940685	-0.054766	4.661010
267.876779	7485.935225	8.945690	-0.054811	4.663437
267.816585	7493.884552	8.950695	-0.054805	4.665836
267.939990	7501.998470	8.955699	-0.054833	4.668284
268.060907	7510.036931	8.960704	-0.054861	4.670707
268.199138	7518.046569	8.965709	-0.054892	4.673120
268.401531	7526.160367	8.970714	-0.054935	4.675563
268.652185	7534.085860	8.975719	-0.054987	4.677949
268.909622	7542.026967	8.980723	-0.055040	4.680337
269.064066	7550.089895	8.985728	-0.055074	4.682762
269.306035	7558.026791	8.990733	-0.055124	4.685146
269.464235	7566.079477	8.995738	-0.055159	4.687565
269.603284	7574.042635	9.000743	-0.055190	4.689956
269.800458	7582.172718	9.005747	-0.055232	4.692395
269.804847	7590.128555	9.010752	-0.055239	4.694781
270.106985	7598.157584	9.015757	-0.055300	4.697187
270.153748	7606.207452	9.020762	-0.055314	4.699599
270.336129	7614.230331	9.025767	-0.055353	4.702001
270.458355	7622.149394	9.030771	-0.055381	4.704371
270.595784	7630.208346	9.035776	-0.055412	4.706781
270.983782	7638.227858	9.040781	-0.055490	4.709178
271.235847	7646.236744	9.045786	-0.055542	4.711571
271.042773	7654.246554	9.050791	-0.055512	4.713964
271.109210	7662.289075	9.055795	-0.055529	4.716365
271.454802	7670.268413	9.060800	-0.055599	4.718744
271.766782	7678.299744	9.065805	-0.055662	4.721139
271.881196	7686.302836	9.070810	-0.055689	4.723524
271.969190	7694.286685	9.075815	-0.055711	4.725902
272.146322	7702.379385	9.080819	-0.055749	4.728312
272.358409	7710.403229	9.085824	-0.055794	4.730699
272.474979	7718.411248	9.090829	-0.055821	4.733081
272.897498	7726.447856	9.095834	-0.055905	4.735469
272.935559	7734.439037	9.100839	-0.055917	4.737843
272.974819	7742.446881	9.105843	-0.055930	4.740222
273.254451	7750.483748	9.110848	-0.055987	4.742607
273.431294	7758.389862	9.115853	-0.056025	4.744952
273.498755	7766.543948	9.120858	-0.056043	4.747370
273.627980	7774.454375	9.125863	-0.056073	4.749714
273.965883	7782.534816	9.130867	-0.056141	4.752107
274.153230	7790.605911	9.135872	-0.056181	4.754496
274.327753	7798.613450	9.140877	-0.056219	4.756865
274.776991	7806.561175	9.145882	-0.056308	4.759215
274.786086	7814.527094	9.150887	-0.056315	4.761570
274.931653	7822.566478	9.155891	-0.056347	4.763945
275.311582	7830.593129	9.160896	-0.056423	4.766314
275.477325	7838.601852	9.165901	-0.056459	4.768678
275.402663	7846.665137	9.170906	-0.056451	4.771058
275.531936	7854.636928	9.175911	-0.056480	4.773408
275.819902	7862.702977	9.180915	-0.056539	4.775785
275.904392	7870.722423	9.185920	-0.056560	4.778147
276.083649	7878.649757	9.190925	-0.056599	4.780481
276.331076	7886.741229	9.195930	-0.056650	4.782861
276.270518	7894.660087	9.200935	-0.056644	4.785191
276.430284	7902.759364	9.205939	-0.056679	4.787572
276.540544	7910.758888	9.210944	-0.056705	4.789923
276.697679	7918.756771	9.215949	-0.056740	4.792271
276.865014	7926.819436	9.220954	-0.056776	4.794638
277.144179	7934.847571	9.225959	-0.056834	4.796992
277.233979	7942.831883	9.230963	-0.056856	4.799334
277.189021	7950.829571	9.235968	-0.056852	4.801679
277.468914	7958.769585	9.240973	-0.056910	4.804004
277.750011	7966.867116	9.245978	-0.056968	4.806374
277.962797	7974.855557	9.250983	-0.057012	4.808712
277.883608	7982.865214	9.255987	-0.057003	4.811056
278.138773	7990.325232	9.260992	-0.057055	4.813236
278.406867	7994.862236	9.265997	-0.057108	4.814561

278.466349	7997.242048	9.271002	-0.057121	4.815257
278.633315	7998.680817	9.276007	-0.057153	4.815676
278.967383	7999.301168	9.281011	-0.057216	4.815856
278.924571	7999.874118	9.286016	-0.057208	4.816023
278.798691	7999.846202	9.291021	-0.057185	4.816016
279.211818	7999.892166	9.296026	-0.057262	4.816027
279.256239	7999.853449	9.301031	-0.057270	4.816015
279.192909	7999.843762	9.306035	-0.057259	4.816013
279.318689	7999.898403	9.311040	-0.057282	4.816028
279.413059	7999.862730	9.316045	-0.057300	4.816017
279.651459	7999.896979	9.321050	-0.057344	4.816026
279.629782	7999.903004	9.326055	-0.057340	4.816028
280.007301	7999.905589	9.331059	-0.057411	4.816027
279.873442	7999.889279	9.336064	-0.057386	4.816023
279.721301	7999.894006	9.341069	-0.057358	4.816025
280.026207	7999.909163	9.346074	-0.057415	4.816028
279.983415	7999.884889	9.351079	-0.057407	4.816021
279.977093	7999.920041	9.356083	-0.057406	4.816031
280.110945	7999.913931	9.361088	-0.057431	4.816029
280.188441	7999.901456	9.366093	-0.057445	4.816025
280.242610	7999.906721	9.371098	-0.057455	4.816026
280.129814	7999.890793	9.376103	-0.057434	4.816022
280.142738	7999.928431	9.381107	-0.057437	4.816033
280.228539	7999.923586	9.386112	-0.057453	4.816031
280.266099	7999.906112	9.391117	-0.057460	4.816025
280.406767	7999.951411	9.396122	-0.057486	4.816038
280.460581	7999.901111	9.401127	-0.057496	4.816023
280.568685	7999.885987	9.406131	-0.057517	4.816018
280.517271	7999.944894	9.411136	-0.057507	4.816035
280.622921	7999.920110	9.416141	-0.057527	4.816028
280.638641	7999.922540	9.421146	-0.057530	4.816028
280.556191	7999.836646	9.426151	-0.057515	4.816004
280.831375	7999.892934	9.431155	-0.057566	4.816019
280.686697	7999.913822	9.436160	-0.057539	4.816025
280.631765	7999.877574	9.441165	-0.057529	4.816015
280.779453	7999.952918	9.446170	-0.057557	4.816036
280.629157	7999.902118	9.451175	-0.057529	4.816022
280.796882	7999.911581	9.456179	-0.057560	4.816024
280.812864	7999.951412	9.461184	-0.057563	4.816036
280.766839	7999.907848	9.466189	-0.057555	4.816023
280.979252	7999.911712	9.471194	-0.057594	4.816023
280.869265	7999.886218	9.476199	-0.057574	4.816016
280.856225	7999.872100	9.481203	-0.057571	4.816012
280.812947	7999.911923	9.486208	-0.057564	4.816024
280.760403	7999.904567	9.491213	-0.057554	4.816022
280.831376	7999.966765	9.496218	-0.057567	4.816040
280.848069	7999.900833	9.501223	-0.057570	4.816021
280.868217	7999.865949	9.506227	-0.057574	4.816010
281.065570	7999.883429	9.511232	-0.057611	4.816015
281.191851	7999.809870	9.516237	-0.057635	4.815992
281.030673	7999.911661	9.521242	-0.057605	4.816023
280.574498	7999.864925	9.526247	-0.057520	4.816012
280.879856	7999.848038	9.531251	-0.057577	4.816005
281.020890	7999.878386	9.536256	-0.057603	4.816013
280.954248	7999.871843	9.541261	-0.057591	4.816012
280.899522	7999.881542	9.546266	-0.057581	4.816015
281.019879	7999.838861	9.551271	-0.057603	4.816002
281.271710	7999.882973	9.556275	-0.057650	4.816013
281.197033	7999.926501	9.561280	-0.057636	4.816026
281.226941	7999.880040	9.566285	-0.057642	4.816013
281.557500	7999.938405	9.571290	-0.057704	4.816028
281.326785	7999.907513	9.576295	-0.057661	4.816020
281.348931	7999.945319	9.581299	-0.057665	4.816031
281.383262	7999.959841	9.586304	-0.057671	4.816035
281.546369	7999.963879	9.591309	-0.057702	4.816035
281.569091	7999.926904	9.596314	-0.057706	4.816025
281.268917	7999.882998	9.601319	-0.057650	4.816013
281.132075	7999.895480	9.606323	-0.057625	4.816018
281.165950	7999.943116	9.611328	-0.057631	4.816031
281.251930	7999.872030	9.616333	-0.057647	4.816010
281.417405	7999.962656	9.621338	-0.057678	4.816036
281.181413	7999.860082	9.626343	-0.057634	4.816007
281.400550	7999.881164	9.631347	-0.057675	4.816012
281.532760	7999.947681	9.636352	-0.057700	4.816031
281.319335	7999.954498	9.641357	-0.057660	4.816034
281.386367	7999.989915	9.646362	-0.057673	4.816044
281.328384	7999.889504	9.651367	-0.057662	4.816015
281.520244	7999.927186	9.656371	-0.057698	4.816025
281.418854	7999.915737	9.661376	-0.057679	4.816022
281.256594	7999.899978	9.666381	-0.057649	4.816018
281.461727	7999.895163	9.671386	-0.057687	4.816016
281.495123	7999.892573	9.676391	-0.057694	4.816015
281.399421	7999.887638	9.681395	-0.057676	4.816014
281.504409	7999.909854	9.686400	-0.057696	4.816020
281.387626	7999.872483	9.691405	-0.057674	4.816010
281.580960	7999.915534	9.696410	-0.057710	4.816021
281.566154	7999.889631	9.701415	-0.057707	4.816014
281.535117	7999.942499	9.706419	-0.057702	4.816029
281.487662	7999.940577	9.711424	-0.057693	4.816029
281.749852	7999.921840	9.716429	-0.057742	4.816022
281.830436	7999.977804	9.721434	-0.057757	4.816038
281.633884	7999.916545	9.726439	-0.057721	4.816021
281.629691	7999.919683	9.731443	-0.057720	4.816022
282.030802	7999.955824	9.736448	-0.057795	4.816030
281.790701	7999.934377	9.741453	-0.057750	4.816025
281.925440	7999.996667	9.746458	-0.057775	4.816043
281.784822	7999.957793	9.751463	-0.057749	4.816032
281.877703	7999.958420	9.756467	-0.057766	4.816032
281.861969	7999.973101	9.761472	-0.057764	4.816036
281.599469	7999.891413	9.766477	-0.057715	4.816014
281.813476	7999.926293	9.771482	-0.057755	4.816023
281.628373	7999.902639	9.776487	-0.057720	4.816017
281.872809	7999.896402	9.781491	-0.057766	4.816014
281.891055	7999.948028	9.786496	-0.057769	4.816029
281.852155	7999.912070	9.791501	-0.057762	4.816019
281.693649	7999.954076	9.796506	-0.057733	4.816032
281.732224	7999.953716	9.801511	-0.057740	4.816031
281.908328	7999.934485	9.806515	-0.057773	4.816025
281.839463	7999.986666	9.811520	-0.057760	4.816040
281.804774	7999.908046	9.816525	-0.057754	4.816018
281.871652	7999.949871	9.821530	-0.057766	4.816030
281.936424	7999.920070	9.826535	-0.057779	4.816020
282.037321	7999.898404	9.831539	-0.057797	4.816014
282.104926	7999.934900	9.836544	-0.057810	4.816024
282.012454	7999.883011	9.841549	-0.057793	4.816009
282.036771	7999.951843	9.846554	-0.057798	4.816029
281.870428	7999.949899	9.851559	-0.057767	4.816030
282.043250	7999.932745	9.856563	-0.057799	4.816024
282.046081	7999.942421	9.861568	-0.057800	4.816026
281.998121	7999.905231	9.866573	-0.057791	4.816016
282.060857	7999.948049	9.871578	-0.057803	4.816028
282.090334	7999.964620	9.876583	-0.057808	4.816033
282.201493	7999.967716	9.881587	-0.057829	4.816033
282.148904	7999.988138	9.886592	-0.057819	4.816039
282.118694	7999.902120	9.891597	-0.057814	4.816014
282.285356	7999.938278	9.896602	-0.057845	4.816024
281.980986	7999.955196	9.901607	-0.057788	4.816030
282.261776	7999.914360	9.906611	-0.057841	4.816017
282.171287	7999.954396	9.911616	-0.057824	4.816029
281.825554	7999.933166	9.916621	-0.057759	4.816025
282.298739	7999.953522	9.921626	-0.057848	4.816028
282.235952	7999.953458	9.926631	-0.057836	4.816029
282.138046	7999.964510	9.931635	-0.057818	4.816032
282.221660	7999.940394	9.936640	-0.057834	4.816025
282.062136	7999.854164	9.941645	-0.057804	4.816000
282.274994	7999.947790	9.946650	-0.057844	4.816027
282.287110	7999.961909	9.951655	-0.057846	4.816031
282.347361	7999.928820	9.956659	-0.057857	4.816021
282.289765	7999.950220	9.961664	-0.057847	4.816027
282.040352	7999.909371	9.966669	-0.057800	4.816017
282.319114	7999.991373	9.971674	-0.057852	4.816039
282.158729	7999.933975	9.976679	-0.057823	4.816023
282.354693	7999.951433	9.981683	-0.057859	4.816027
282.165178	7999.975780	9.986688	-0.057824	4.816035
282.226031	7999.912785	9.991693	-0.057835	4.816017
282.127366	7999.923823	9.996698	-0.057817	4.816020
282.137824	7999.910131	10.001703	-0.057819	4.816016
282.083457	7999.966850	10.006707	-0.057809	4.816033
282.355621	7999.965391	10.011712	-0.057860	4.816031
282.164095	7999.965126	10.016717	-0.057824	4.816032
282.394512	7999.989621	10.021722	-0.057867	4.816038
282.434611	7999.988221	10.026727	-0.057875	4.816038
282.386950	7999.970267	10.031731	-0.057866	4.816033
282.296308	7999.994273	10.036736	-0.057849	4.816040
282.422724	7999.934605	10.041741	-0.057873	4.816022
282.478069	7999.993318	10.046746	-0.057883	4.816039
282.384927	7999.960648	10.051751	-0.057866	4.816030
282.546110	7999.960379	10.056755	-0.057896	4.816029
282.521675	7999.983450	10.061760	-0.057892	4.816036
282.421756	7999.978438	10.066765	-0.057873	4.816035
282.495577	8000.012910	10.071770	-0.057887	4.816045
282.464760	7999.965345	10.076775	-0.057881	4.816031
282.368007	7999.968939	10.081779	-0.057863	4.816032
282.424302	7999.980655	10.086784	-0.057874	4.816035
282.625039	7999.974693	10.091789	-0.057911	4.816033
282.556829	8000.019408	10.096794	-0.057899	4.816046
282.456804	7999.962037	10.101799	-0.057880	4.816030
282.558031	8000.010898	10.106803	-0.057899	4.816044
282.605045	8000.002144	10.111808	-0.057908	4.816041
282.379487	7999.987370	10.116813	-0.057866	4.816038
282.503223	8000.012065	10.121818	-0.057889	4.816044
282.656723	7999.983875	10.126823	-0.057918	4.816035
282.711929	8000.007325	10.131827	-0.057928	4.816042
282.824091	8000.015782	10.136832	-0.057949	4.816044
282.822978	7999.954866	10.141837	-0.057949	4.816026
282.852257	8000.005626	10.146842	-0.057955	4.816040
282.695798	7999.941887	10.151847	-0.057926	4.816023
282.775932	7999.998913	10.156851	-0.057941	4.816039
282.698549	8000.007132	10.161856	-0.057926	4.816042
282.706733	7999.977372	10.166861	-0.057928	4.816033
282.750487	7999.994202	10.171866	-0.057936	4.816038
282.725000	7999.951008	10.176871	-0.057931	4.816025
282.807675	7999.978162	10.181875	-0.057947	4.816033
282.772443	8000.009585	10.186880	-0.057940	4.816042
282.728087	7999.983144	10.191885	-0.057932	4.816035
282.748403	8000.012371	10.196890	-0.057936	4.816043
282.564411	8000.022927	10.201895	-0.057902	4.816047
282.432371	8000.048317	10.206899	-0.057878	4.816055
282.535203	8000.005317	10.211904	-0.057897	4.816042
282.544030	7999.956335	10.216909	-0.057898	4.816028
282.607900	7999.967120	10.221914	-0.057910	4.816030
282.877818	7999.956005	10.226919	-0.057961	4.816026
282.983643	7999.985717	10.231923	-0.057981	4.816034
282.729661	7999.992864	10.236928	-0.057933	4.816037
282.794448	7999.981228	10.241933	-0.057945	4.816034
282.860683	7999.997399	10.246938	-0.057958	4.816038
282.694988	7999.990123	10.251943	-0.057927	4.816037
282.886144	8000.004289	10.256947	-0.057963	4.816040
282.998818	7999.993523	10.261952	-0.057984	4.816036
282.926832	7999.986881	10.266957	-0.057971	4.816035
282.700761	7999.976371	10.271962	-0.057929	4.816033
282.680730	7999.968536	10.276967	-0.057925	4.816030
282.869386	7999.970903	10.281971	-0.057960	4.816030
282.796797	8000.001648	10.286976	-0.057947	4.816040
282.812196	7999.961333	10.291981	-0.057950	4.816028
283.054371	8000.002070	10.296986	-0.057995	4.816038
283.004450	7999.971254	10.301991	-0.057986	4.816030
282.984872	7999.938851	10.306995	-0.057982	4.816020
283.035655	7999.991070	10.312000	-0.057992	4.816035
282.921137	7999.980450	10.317005	-0.057970	4.816033
282.950304	8000.025866	10.322010	-0.057976	4.816046
283.007860	8000.006618	10.327015	-0.057987	4.816040
283.020751	8000.016477	10.332019	-0.057989	4.816043
282.968993	8000.016614	10.337024	-0.057980	4.816043
282.989930	7999.995632	10.342029	-0.057984	4.816037
283.050783	8000.022391	10.347034	-0.057995	4.816044
283.081690	7999.997317	10.352039	-0.058001	4.816037
283.066180	8000.015208	10.357043	-0.057998	4.816042
283.079094	8000.026136	10.362048	-0.058001	4.816045
283.042129	8000.006239	10.367053	-0.057994	4.816040
283.056248	8000.024669	10.372058	-0.057997	4.816045
282.981743	7999.989131	10.377063	-0.057983	4.816035
283.199945	8000.000584	10.382067	-0.058023	4.816037
283.210924	8000.010409	10.387072	-0.058026	4.816040
282.952451	7999.968323	10.392077	-0.057977	4.816029
283.098219	8000.023337	10.397082	-0.058005	4.816044
283.142744	7999.962181	10.402087	-0.058013	4.816026
283.048110	7999.996799	10.407091	-0.057996	4.816037
283.070431	7999.991870	10.412096	-0.058000	4.816035
282.803602	7999.979551	10.417101	-0.057950	4.816033
282.861226	8000.015867	10.422106	-0.057961	4.816043
282.907039	8000.013502	10.427111	-0.057970	4.816042
282.982169	8000.018081	10.432115	-0.057984	4.816043
282.892856	7999.999371	10.437120	-0.057967	4.816038
282.724365	7999.952509	10.442125	-0.057936	4.816025
283.081151	8000.010288	10.447130	-0.058002	4.816040
283.019509	7999.960025	10.452135	-0.057991	4.816026
283.162279	7999.905997	10.457139	-0.058018	4.816010
283.180122	7999.983262	10.462144	-0.058021	4.816032
283.028618	8000.000819	10.467149	-0.057993	4.816038
283.245117	8000.034680	10.472154	-0.058033	4.816047
283.212875	7999.997773	10.477159	-0.058027	4.816036
283.162048	7999.986173	10.482163	-0.058018	4.816033
283.325566	7999.992358	10.487168	-0.058049	4.816034
283.217204	7999.929492	10.492173	-0.058028	4.816016
283.388701	8000.013824	10.497178	-0.058061	4.816040
283.207422	7999.990236	10.502183	-0.058027	4.816034
283.167441	7999.963874	10.507187	-0.058019	4.816026
283.108400	7999.971358	10.512192	-0.058009	4.816029
283.126972	7999.982389	10.517197	-0.058012	4.816032
283.131121	7999.982472	10.522202	-0.058013	4.816032
282.951332	7999.952501	10.527207	-0.057980	4.816024
283.217691	7999.932774	10.532211	-0.058029	4.816017
283.144024	7999.987006	10.537216	-0.058016	4.816033
283.027762	7999.950710	10.542221	-0.057994	4.816023
283.293732	7999.959825	10.547226	-0.058044	4.816025
283.328654	7999.955125	10.552231	-0.058050	4.816023
283.169414	7999.907363	10.557235	-0.058021	4.816010
283.156101	7999.948801	10.562240	-0.058018	4.816022
283.116049	7999.927780	10.567245	-0.058011	4.816016
283.433735	8000.011563	10.572250	-0.058070	4.816039
283.127356	7999.988907	10.577255	-0.058013	4.816034
283.301914	7999.962169	10.582259	-0.058046	4.816025
283.487086	8000.001872	10.587264	-0.058080	4.816036
283.187211	7999.962239	10.592269	-0.058025	4.816026
283.301929	7999.973948	10.597274	-0.058046	4.816029
283.326571	7999.979747	10.602279	-0.058051	4.816030
283.411892	7999.969552	10.607283	-0.058067	4.816027
283.426056	8000.012559	10.612288	-0.058069	4.816039
283.430713	8000.009446	10.617293	-0.058070	4.816038
283.307921	8000.005086	10.622298	-0.058048	4.816038
283.348180	7999.987661	10.627303	-0.058055	4.816032
283.308528	7999.979470	10.632307	-0.058048	4.816030
283.155003	7999.998058	10.637312	-0.058019	4.816036
283.208503	7999.985148	10.642317	-0.058029	4.816032
283.437741	7999.972226	10.647322	-0.058072	4.816027
283.449954	7999.973525	10.652327	-0.058075	4.816028
283.168425	7999.962007	10.657331	-0.058022	4.816026
283.314807	7999.991388	10.662336	-0.058050	4.816034
283.478763	7999.969800	10.667341	-0.058080	4.816026
283.369267	8000.013764	10.672346	-0.058060	4.816040
283.454521	8000.007843	10.677351	-0.058076	4.816038
283.357640	8000.010364	10.682355	-0.058058	4.816039
283.418456	8000.017889	10.687360	-0.058069	4.816041
283.304058	7999.958119	10.692365	-0.058048	4.816024
283.264589	8000.024726	10.697370	-0.058041	4.816044
283.241715	7999.991195	10.702375	-0.058037	4.816034
283.306913	7999.989183	10.707379	-0.058049	4.816033
283.362074	7999.988056	10.712384	-0.058059	4.816032
283.355924	7999.951624	10.717389	-0.058058	4.816022
283.556802	7999.994818	10.722394	-0.058096	4.816033
283.256643	7999.984029	10.727399	-0.058040	4.816032
283.290731	7999.970766	10.732403	-0.058046	4.816028
283.297627	7999.986927	10.737408	-0.058048	4.816032
283.211469	7999.965068	10.742413	-0.058032	4.816026
283.221257	8000.000515	10.747418	-0.058034	4.816037
283.303581	7999.985992	10.752423	-0.058049	4.816032
283.211944	7999.995020	10.757427	-0.058032	4.816035
283.174316	8000.029606	10.762432	-0.058025	4.816045
283.004051	7999.898300	10.767437	-0.057993	4.816008
283.358611	7999.956039	10.772442	-0.058060	4.816023
283.292526	7999.984765	10.777447	-0.058047	4.816032
283.038047	7999.976943	10.782451	-0.058000	4.816031
283.354591	8000.005143	10.787456	-0.058059	4.816037
283.322514	7999.951142	10.792461	-0.058053	4.816022
283.354248	8000.011564	10.797466	-0.058059	4.816039
283.229498	8000.005032	10.802471	-0.058036	4.816038
283.371464	7999.978770	10.807475	-0.058063	4.816030
283.482222	8000.006435	10.812480	-0.058083	4.816037
283.592396	7999.991350	10.817485	-0.058104	4.816032
283.506477	7999.975906	10.822490	-0.058088	4.816028
283.437822	7999.968256	10.827495	-0.058075	4.816026
283.497343	8000.001401	10.832499	-0.058087	4.816035
283.511297	8000.029445	10.837504	-0.058089	4.816044
283.223207	8000.013532	10.842509	-0.058036	4.816040
283.412802	8000.009507	10.847514	-0.058071	4.816038
283.528732	7999.936826	10.852519	-0.058093	4.816016
283.651189	7999.960430	10.857523	-0.058116	4.816023
283.417768	7999.998937	10.862528	-0.058072	4.816035
283.424054	7999.972347	10.867533	-0.058073	4.816027
283.535339	8000.013913	10.872538	-0.058094	4.816039
283.407023	8000.008383	10.877543	-0.058070	4.816038
283.395667	7999.977199	10.882547	-0.058068	4.816029
283.309876	8000.000224	10.887552	-0.058053	4.816036
283.495657	7999.963005	10.892557	-0.058087	4.816024
283.649531	8000.022441	10.897562	-0.058116	4.816041
283.428205	7999.995988	10.902567	-0.058075	4.816034
283.501555	8000.008015	10.907571	-0.058089	4.816037
283.530785	8000.035267	10.912576	-0.058094	4.816045
283.501241	7999.990930	10.917581	-0.058089	4.816032
283.635543	8000.021160	10.922586	-0.058114	4.816040
283.395737	7999.997577	10.927591	-0.058069	4.816035
283.545098	7999.976793	10.932595	-0.058097	4.816028
283.749378	8000.006158	10.937600	-0.058135	4.816035
283.725526	7999.997185	10.942605	-0.058131	4.816033
283.555883	7999.972740	10.947610	-0.058099	4.816027
283.440904	7999.981344	10.952615	-0.058078	4.816030
283.603644	7999.985378	10.957619	-0.058108	4.816030
283.564161	8000.003902	10.962624	-0.058101	4.816036
283.448239	7999.975091	10.967629	-0.058080	4.816028
283.630484	7999.997645	10.972634	-0.058114	4.816034
283.432683	8000.016497	10.977639	-0.058077	4.816040
283.507604	7999.991154	10.982643	-0.058091	4.816032
283.513254	8000.026527	10.987648	-0.058092	4.816043
283.387938	7999.941982	10.992653	-0.058069	4.816019
283.479869	8000.012046	10.997658	-0.058086	4.816039
283.400233	7999.990305	11.002663	-0.058071	4.816033
283.472146	8000.008717	11.007667	-0.058085	4.816038
283.516596	8000.028766	11.012672	-0.058093	4.816043
283.402519	7999.981824	11.017677	-0.058072	4.816030
283.650178	8000.020526	11.022682	-0.058118	4.816040
283.380923	7999.989996	11.027687	-0.058068	4.816033
283.484754	7999.960904	11.032691	-0.058088	4.816024
283.644811	8000.020453	11.037696	-0.058118	4.816040
283.534925	7999.988546	11.042701	-0.058097	4.816031
283.454673	8000.023425	11.047706	-0.058082	4.816042
283.446284	7999.997637	11.052711	-0.058081	4.816035
283.702891	7999.994829	11.057715	-0.058129	4.816032
283.621447	7999.988015	11.062720	-0.058114	4.816031
283.546662	7999.965294	11.067725	-0.058100	4.816025
283.506685	8000.005179	11.072730	-0.058092	4.816036
283.616294	8000.016797	11.077735	-0.058113	4.816039
283.394134	8000.026658	11.082739	-0.058072	4.816043
283.606116	8000.026245	11.087744	-0.058111	4.816042
283.636124	8000.003291	11.092749	-0.058117	4.816035
283.501794	8000.016886	11.097754	-0.058092	4.816040
283.493761	7999.994310	11.102759	-0.058091	4.816033
283.479479	7999.998333	11.107763	-0.058088	4.816035
283.575208	8000.001149	11.112768	-0.058106	4.816035
283.618629	8000.000878	11.117773	-0.058114	4.816035
283.675299	8000.062823	11.122778	-0.058125	4.816052
283.653767	8000.004739	11.127783	-0.058121	4.816035
283.705489	7999.953330	11.132787	-0.058130	4.816020
283.774524	8000.008019	11.137792	-0.058143	4.816036
283.645373	7999.978967	11.142797	-0.058119	4.816028
283.581998	8000.049415	11.147802	-0.058108	4.816049
283.609832	8000.033901	11.152807	-0.058113	4.816044
283.745683	8000.040653	11.157811	-0.058138	4.816045
283.789337	8000.011536	11.162816	-0.058147	4.816037
283.662135	7999.964355	11.167821	-0.058123	4.816024
283.813270	8000.020536	11.172826	-0.058151	4.816039
283.729832	7999.999795	11.177831	-0.058136	4.816034
283.551144	8000.029679	11.182835	-0.058103	4.816043
283.727689	8000.041445	11.187840	-0.058136	4.816046
283.714604	8000.002749	11.192845	-0.058133	4.816035
283.921631	8000.033233	11.197850	-0.058172	4.816042
283.773274	7999.982461	11.202855	-0.058144	4.816028
283.741803	8000.032118	11.207859	-0.058139	4.816043
283.875053	8000.040960	11.212864	-0.058163	4.816045
283.792738	7999.991388	11.217869	-0.058148	4.816031
283.722354	8000.021105	11.222874	-0.058135	4.816040
283.960716	8000.028651	11.227879	-0.058180	4.816041
283.915840	8000.001131	11.232883	-0.058171	4.816033
283.883553	8000.036882	11.237888	-0.058165	4.816044
283.772421	7999.979307	11.242893	-0.058145	4.816027
283.923698	8000.002367	11.247898	-0.058173	4.816033
283.670214	8000.024481	11.252903	-0.058126	4.816041
283.755677	7999.951246	11.257907	-0.058142	4.816019
283.787831	8000.004197	11.262912	-0.058148	4.816035
283.782257	7999.997693	11.267917	-0.058147	4.816033
283.804425	7999.984213	11.272922	-0.058151	4.816029
283.927181	7999.989659	11.277927	-0.058174	4.816030
283.865090	8000.000292	11.282931	-0.058163	4.816033
283.905252	8000.033087	11.287936	-0.058170	4.816042
283.932009	8000.026102	11.292941	-0.058175	4.816040
283.893154	8000.052117	11.297946	-0.058168	4.816048
283.989676	8000.015413	11.302951	-0.058186	4.816037
283.855641	8000.004437	11.307955	-0.058161	4.816034
283.957885	8000.009509	11.312960	-0.058181	4.816035
283.846417	7999.995737	11.317965	-0.058160	4.816032
284.104606	8000.027152	11.322970	-0.058208	4.816040
283.967267	8000.032144	11.327975	-0.058183	4.816042
283.890974	8000.021149	11.332979	-0.058168	4.816039
283.802083	8000.038775	11.337984	-0.058152	4.816045
283.831508	8000.002988	11.342989	-0.058158	4.816034
284.053408	8000.035880	11.347994	-0.058199	4.816042
283.910567	8000.033292	11.352999	-0.058172	4.816042
283.979242	8000.003562	11.358003	-0.058185	4.816033
284.193582	8000.055551	11.363008	-0.058225	4.816047
283.916139	8000.021665	11.368013	-0.058174	4.816039
283.821740	8000.033848	11.373018	-0.058156	4.816043
284.000392	8000.064886	11.378023	-0.058190	4.816051
283.864729	8000.047469	11.383027	-0.058164	4.816047
283.843849	8000.027864	11.388032	-0.058161	4.816041
283.865355	8000.001550	11.393037	-0.058165	4.816033
284.028563	8000.044061	11.398042	-0.058195	4.816045
283.864888	8000.013312	11.403047	-0.058165	4.816037
283.697939	7999.989984	11.408051	-0.058134	4.816031
283.902841	8000.036458	11.413056	-0.058172	4.816043
283.877994	7999.990068	11.418061	-0.058167	4.816030
283.881540	8000.012580	11.423066	-0.058168	4.816036
283.831997	8000.008482	11.428071	-0.058159	4.816035
283.944080	7999.994500	11.433075	-0.058180	4.816031
283.974639	7999.993995	11.438080	-0.058186	4.816030
283.746270	7999.988784	11.443085	-0.058143	4.816030
283.900200	8000.032195	11.448090	-0.058172	4.816042
283.729150	8000.013066	11.453095	-0.058140	4.816037
283.813857	7999.991106	11.458099	-0.058156	4.816030
283.853866	8000.037789	11.463104	-0.058164	4.816044
283.821070	7999.979501	11.468109	-0.058158	4.816027
283.895268	8000.025736	11.473114	-0.058172	4.816040
283.862278	8000.023007	11.478119	-0.058166	4.816040
283.977632	8000.010153	11.483123	-0.058187	4.816035
283.767368	8000.004203	11.488128	-0.058148	4.816035
283.768381	7999.987133	11.493133	-0.058148	4.816030
284.043957	8000.021001	11.498138	-0.058200	4.816038
284.030147	7999.987634	11.503143	-0.058197	4.816028
283.871719	7999.947364	11.508147	-0.058168	4.816017
283.990613	8000.000823	11.513152	-0.058190	4.816032
283.918571	7999.965329	11.518157	-0.058177	4.816022
283.906089	8000.031359	11.523162	-0.058175	4.816042
283.877140	8000.019087	11.528167	-0.058169	4.816038
284.016022	8000.005592	11.533171	-0.058195	4.816034
284.108559	8000.022242	11.538176	-0.058212	4.816038
284.119698	8000.008562	11.543181	-0.058215	4.816034
284.003679	8000.029970	11.548186	-0.058193	4.816041
283.923164	8000.012486	11.553191	-0.058178	4.816036
284.048027	7999.992325	11.558195	-0.058202	4.816030
284.271517	8000.049823	11.563200	-0.058243	4.816045
284.076560	7999.989655	11.568205	-0.058207	4.816029
284.129862	8000.018414	11.573210	-0.058217	4.816037
284.072127	8000.004551	11.578215	-0.058206	4.816033
284.000915	8000.001128	11.583219	-0.058193	4.816032
284.010393	8000.028022	11.588224	-0.058195	4.816040
283.916758	8000.016711	11.593229	-0.058178	4.816037
283.976234	8000.025280	11.598234	-0.058189	4.816040
284.076771	8000.031391	11.603239	-0.058208	4.816041
284.025039	7999.979169	11.608243	-0.058198	4.816026
283.866641	8000.020108	11.613248	-0.058169	4.816039
283.976894	7999.990064	11.618253	-0.058189	4.816029
284.138347	8000.017584	11.623258	-0.058219	4.816036
283.788272	8000.001612	11.628263	-0.058154	4.816034
284.061490	7999.975599	11.633267	-0.058205	4.816025
284.107389	8000.045897	11.638272	-0.058214	4.816045
283.847674	8000.006991	11.643277	-0.058166	4.816035
284.214187	8000.032896	11.648282	-0.058234	4.816040
284.018796	8000.006913	11.653287	-0.058198	4.816034
284.029307	8000.023140	11.658291	-0.058200	4.816039
284.034604	8000.031793	11.663296	-0.058201	4.816041
284.066664	8000.006740	11.668301	-0.058207	4.816034
283.946648	8000.024868	11.673306	-0.058185	4.816040
283.963690	8000.001679	11.678311	-0.058188	4.816033
284.132106	8000.007954	11.683315	-0.058219	4.816034
284.330246	8000.047895	11.688320	-0.058256	4.816044
284.101573	7999.949715	11.693325	-0.058214	4.816017
284.097747	7999.997738	11.698330	-0.058213	4.816031
284.112704	8000.038623	11.703335	-0.058216	4.816043
284.159602	8000.025593	11.708339	-0.058225	4.816039
284.186206	8000.039976	11.713344	-0.058230	4.816043
284.149252	7999.994434	11.718349	-0.058223	4.816030
284.050137	8000.014011	11.723354	-0.058205	4.816036
284.150465	8000.012638	11.728359	-0.058224	4.816035
284.019020	7999.987818	11.733363	-0.058199	4.816028
284.189672	8000.044355	11.738368	-0.058231	4.816044
284.114669	7999.993847	11.743373	-0.058217	4.816030
283.931908	7999.996945	11.748378	-0.058183	4.816031
284.141944	8000.006114	11.753383	-0.058222	4.816033
283.930738	8000.022585	11.758387	-0.058183	4.816039
284.158008	8000.070535	11.763392	-0.058226	4.816052
284.003274	7999.963014	11.768397	-0.058197	4.816021
284.040513	7999.985070	11.773402	-0.058204	4.816027
284.043419	8000.003296	11.778407	-0.058204	4.816033
284.143448	7999.997643	11.783411	-0.058223	4.816030
284.039513	8000.039572	11.788416	-0.058204	4.816043
283.826892	8000.041058	11.793421	-0.058164	4.816045
283.982623	8000.034281	11.798426	-0.058194	4.816042
283.992030	8000.029117	11.803431	-0.058195	4.816040
284.009692	8000.030515	11.808435	-0.058199	4.816041
284.075549	8000.042406	11.813440	-0.058211	4.816044
284.015958	8000.005001	11.818445	-0.058200	4.816033
284.241970	8000.023009	11.823450	-0.058242	4.816037
284.052548	8000.020643	11.828455	-0.058207	4.816038
283.893166	8000.006000	11.833459	-0.058177	4.816034
284.205081	8000.054420	11.838464	-0.058236	4.816047
284.089534	8000.023477	11.843469	-0.058214	4.816038
284.126256	8000.028427	11.848474	-0.058221	4.816040
284.024406	8000.051160	11.853479	-0.058202	4.816047
283.828491	7999.995249	11.858483	-0.058166	4.816031
284.051887	8000.019621	11.863488	-0.058208	4.816037
284.090234	8000.002161	11.868493	-0.058215	4.816032
284.043524	8000.064364	11.873498	-0.058206	4.816050
283.977342	8000.008674	11.878503	-0.058194	4.816035
284.043057	8000.016288	11.883507	-0.058206	4.816036
284.233412	8000.042196	11.888512	-0.058242	4.816043
283.936266	8000.023980	11.893517	-0.058186	4.816039
283.895828	8000.060652	11.898522	-0.058179	4.816050
284.114872	8000.041135	11.903527	-0.058220	4.816043
284.053858	8000.043240	11.908531	-0.058209	4.816044
283.954497	8000.021140	11.913536	-0.058190	4.816038
284.176793	7999.985653	11.918541	-0.058232	4.816027
284.210024	8000.059995	11.923546	-0.058238	4.816048
284.163149	8000.049535	11.928551	-0.058229	4.816045
284.023871	8000.039531	11.933555	-0.058204	4.816043
284.390997	8000.084682	11.938560	-0.058272	4.816054
284.341765	8000.029299	11.943565	-0.058263	4.816039
284.041677	8000.035606	11.948570	-0.058207	4.816042
284.205652	7999.993717	11.953575	-0.058238	4.816029
284.241053	7999.956970	11.958579	-0.058244	4.816018
284.297049	7999.994326	11.963584	-0.058255	4.816029
284.030717	7999.989493	11.968589	-0.058205	4.816029
284.379031	8000.020410	11.973594	-0.058270	4.816036
284.173303	7999.998513	11.978599	-0.058232	4.816030
284.112278	7999.996344	11.983603	-0.058221	4.816030
284.266811	8000.039766	11.988608	-0.058250	4.816042
284.024816	7999.975537	11.993613	-0.058205	4.816025
284.116260	7999.982550	11.998618	-0.058222	4.816026
284.094916	8000.005678	12.003623	-0.058218	4.816033
284.200726	8000.002268	12.008627	-0.058238	4.816031
284.204632	8000.049363	12.013632	-0.058239	4.816045
284.037178	8000.005723	12.018637	-0.058207	4.816033
284.043849	8000.041114	12.023642	-0.058209	4.816044
284.160921	8000.031497	12.028647	-0.058231	4.816040
284.143281	8000.036527	12.033651	-0.058227	4.816042
284.131091	8000.056616	12.038656	-0.058225	4.816048
284.143634	8000.031208	12.043661	-0.058228	4.816040
284.160818	8000.072133	12.048666	-0.058231	4.816052
284.248594	8000.049161	12.053671	-0.058247	4.816045
284.187057	8000.028817	12.058675	-0.058236	4.816039
284.180326	8000.045799	12.063680	-0.058235	4.816044
284.113392	8000.002918	12.068685	-0.058222	4.816032
284.076072	8000.047126	12.073690	-0.058216	4.816045
284.031099	8000.047386	12.078695	-0.058207	4.816045
283.992124	8000.017835	12.083699	-0.058200	4.816037
284.314693	8000.038667	12.088704	-0.058260	4.816041
284.149687	8000.021785	12.093709	-0.058230	4.816037
284.109047	8000.056316	12.098714	-0.058222	4.816048
284.124311	8000.061945	12.103719	-0.058225	4.816049
284.358171	8000.045903	12.108723	-0.058269	4.816043
284.304750	8000.064174	12.113728	-0.058259	4.816049
284.125631	8000.022458	12.118733	-0.058226	4.816038
284.170217	8000.056402	12.123738	-0.058234	4.816047
284.109379	8000.023248	12.128743	-0.058223	4.816038
284.174244	7999.944295	12.133747	-0.058235	4.816015
284.166182	7999.997584	12.138752	-0.058234	4.816030
284.389406	7999.988828	12.143757	-0.058275	4.816026
284.553643	8000.029221	12.148762	-0.058306	4.816037
284.514702	8000.049893	12.153767	-0.058299	4.816044
284.305078	8000.055707	12.158771	-0.058260	4.816046
284.313890	8000.048395	12.163776	-0.058261	4.816044
284.222328	7999.998655	12.168781	-0.058244	4.816030
284.304595	8000.022598	12.173786	-0.058260	4.816037
284.136437	8000.007796	12.178791	-0.058229	4.816033
284.066772	7999.989441	12.183795	-0.058216	4.816028
284.175000	8000.066215	12.188800	-0.058236	4.816050
284.302082	8000.018312	12.193805	-0.058260	4.816035
284.302972	8000.029022	12.198810	-0.058260	4.816039
284.346445	8000.028752	12.203815	-0.058268	4.816038
284.553589	8000.063515	12.208819	-0.058307	4.816047
284.614629	8000.066770	12.213824	-0.058318	4.816048
284.308890	8000.040917	12.218829	-0.058261	4.816042
284.311684	8000.061279	12.223834	-0.058262	4.816048
284.389521	8000.056291	12.228839	-0.058277	4.816046
284.306656	8000.014188	12.233843	-0.058261	4.816034
284.477775	8000.034404	12.238848	-0.058293	4.816039
284.486208	8000.030292	12.243853	-0.058295	4.816038
284.409825	8000.059899	12.248858	-0.058281	4.816047
284.301138	8000.060069	12.253863	-0.058261	4.816048
284.261632	8000.047605	12.258867	-0.058253	4.816044
284.272098	8000.061695	12.263872	-0.058255	4.816048
284.050053	8000.015993	12.268877	-0.058214	4.816036
284.474389	8000.055773	12.273882	-0.058293	4.816045
284.401348	8000.036288	12.278887	-0.058280	4.816040
284.238149	8000.019438	12.283891	-0.058249	4.816036
284.190630	8000.050639	12.288896	-0.058241	4.816045
284.382096	8000.013523	12.293901	-0.058276	4.816034
284.445689	8000.028579	12.298906	-0.058288	4.816038
284.503122	8000.029632	12.303911	-0.058299	4.816038
284.302368	8000.038813	12.308915	-0.058262	4.816041
284.629807	8000.053323	12.313920	-0.058323	4.816044
284.200157	8000.002778	12.318925	-0.058243	4.816031
284.256442	8000.047620	12.323930	-0.058254	4.816044
284.435685	8000.066915	12.328935	-0.058287	4.816049
284.406587	8000.052503	12.333939	-0.058282	4.816045
284.374932	8000.072239	12.338944	-0.058276	4.816051
284.384979	8000.026482	12.343949	-0.058278	4.816037
284.505991	7999.991292	12.348954	-0.058300	4.816026
284.400878	7999.995800	12.353959	-0.058281	4.816028
284.450493	7999.992437	12.358963	-0.058290	4.816027
284.413846	8000.023835	12.363968	-0.058284	4.816036
284.483397	8000.005874	12.368973	-0.058297	4.816031
284.476203	8000.020711	12.373978	-0.058295	4.816035
284.513573	8000.027810	12.378983	-0.058302	4.816037
284.310603	8000.011306	12.383987	-0.058265	4.816033
284.642360	8000.041923	12.388992	-0.058326	4.816040
284.565292	8000.035187	12.393997	-0.058312	4.816039
284.490974	8000.013542	12.399002	-0.058298	4.816033
284.432532	8000.029585	12.404007	-0.058288	4.816038
284.474819	7999.979072	12.409011	-0.058296	4.816023
284.496535	8000.027559	12.414016	-0.058300	4.816037
284.325492	8000.006293	12.419021	-0.058268	4.816032
284.246841	8000.010214	12.424026	-0.058253	4.816033
284.525198	8000.050545	12.429031	-0.058305	4.816044
284.600257	8000.030548	12.434035	-0.058319	4.816037
284.333102	8000.051344	12.439040	-0.058270	4.816045
284.250813	8000.009251	12.444045	-0.058255	4.816033
284.295679	8000.052817	12.449050	-0.058263	4.816045
284.326953	8000.005310	12.454055	-0.058269	4.816031
284.393341	7999.992634	12.459059	-0.058281	4.816027
284.484392	8000.022080	12.464064	-0.058298	4.816035
284.297900	7999.990915	12.469069	-0.058264	4.816027
284.362601	7999.966455	12.474074	-0.058276	4.816020
284.301685	8000.015578	12.479079	-0.058265	4.816035
284.368380	7999.982605	12.484083	-0.058277	4.816025
284.406364	8000.023909	12.489088	-0.058284	4.816036
284.428199	8000.008286	12.494093	-0.058288	4.816032
284.365843	8000.005024	12.499098	-0.058277	4.816031
284.328219	8000.023582	12.504103	-0.058270	4.816037
284.485184	7999.970880	12.509107	-0.058299	4.816020
284.641416	8000.037842	12.514112	-0.058328	4.816039
284.561807	7999.978701	12.519117	-0.058314	4.816022
284.499757	8000.022460	12.524122	-0.058302	4.816035
284.638141	8000.023916	12.529127	-0.058328	4.816035
284.685267	8000.020507	12.534131	-0.058337	4.816034
284.662415	8000.062842	12.539136	-0.058333	4.816046
284.583569	8000.025086	12.544141	-0.058318	4.816036
284.446320	8000.026873	12.549146	-0.058293	4.816037
284.455319	8000.040936	12.554151	-0.058295	4.816041
284.332249	8000.018405	12.559155	-0.058272	4.816035
284.394169	8000.069761	12.564160	-0.058283	4.816050
284.431906	8000.046947	12.569165	-0.058290	4.816043
284.360092	8000.065952	12.574170	-0.058277	4.816049
284.418861	8000.037110	12.579175	-0.058288	4.816040
284.500343	8000.016160	12.584179	-0.058303	4.816034
284.513859	8000.027100	12.589184	-0.058306	4.816037
284.326772	8000.046146	12.594189	-0.058271	4.816043
284.345483	8000.070003	12.599194	-0.058275	4.816050
284.331417	8000.056933	12.604199	-0.058272	4.816046
284.473911	8000.022133	12.609203	-0.058299	4.816035
284.554419	8000.032153	12.614208	-0.058314	4.816038
284.629149	8000.008944	12.619213	-0.058328	4.816031
284.589157	8000.038145	12.624218	-0.058321	4.816040
284.424431	8000.045843	12.629223	-0.058290	4.816043
284.497851	7999.977731	12.634227	-0.058304	4.816022
284.508669	8000.055940	12.639232	-0.058306	4.816045
284.400030	8000.034739	12.644237	-0.058286	4.816040
284.739422	8000.047330	12.649242	-0.058349	4.816041
284.700114	8000.045555	12.654247	-0.058342	4.816041
284.454081	8000.012239	12.659251	-0.058296	4.816033
284.501900	8000.065476	12.664256	-0.058305	4.816048
284.500162	8000.003477	12.669261	-0.058305	4.816030
284.557236	8000.062225	12.674266	-0.058316	4.816047
284.662792	8000.064153	12.679271	-0.058335	4.816047
284.622081	8000.014267	12.684275	-0.058328	4.816032
284.492511	8000.052525	12.689280	-0.058304	4.816044
284.351335	8000.015773	12.694285	-0.058278	4.816034
284.571528	8000.057184	12.699290	-0.058319	4.816045
284.941289	8000.060711	12.704295	-0.058388	4.816044
284.615813	8000.037703	12.709299	-0.058327	4.816039
284.603982	8000.052456	12.714304	-0.058325	4.816044
284.592270	8000.047978	12.719309	-0.058323	4.816042
284.647110	8000.026544	12.724314	-0.058333	4.816036
284.758991	8000.040341	12.729319	-0.058354	4.816039
284.729009	8000.038735	12.734323	-0.058349	4.816039
284.728862	8000.031261	12.739328	-0.058349	4.816037
284.507884	8000.010155	12.744333	-0.058308	4.816032
284.727736	8000.044080	12.749338	-0.058349	4.816040
284.654231	8000.044889	12.754343	-0.058335	4.816041
284.597495	8000.007535	12.759347	-0.058324	4.816030
284.738095	8000.049636	12.764352	-0.058351	4.816042
284.584929	8000.040448	12.769357	-0.058322	4.816040
284.534312	8000.028851	12.774362	-0.058313	4.816037
284.544018	8000.005528	12.779367	-0.058315	4.816030
284.629440	7999.981444	12.784371	-0.058331	4.816023
284.653895	8000.040667	12.789376	-0.058336	4.816040
284.448336	8000.038007	12.794381	-0.058297	4.816040
284.792275	8000.061366	12.799386	-0.058361	4.816045
284.807565	8000.074475	12.804391	-0.058364	4.816049
284.555847	8000.048535	12.809395	-0.058318	4.816043
284.609515	8000.077302	12.814400	-0.058328	4.816051
284.546485	8000.056930	12.819405	-0.058316	4.816045
284.629209	8000.070197	12.824410	-0.058332	4.816049
284.674179	8000.046446	12.829415	-0.058340	4.816041
284.654616	8000.017248	12.834419	-0.058336	4.816033
284.807708	8000.038206	12.839424	-0.058365	4.816038
284.514289	8000.032878	12.844429	-0.058310	4.816038
284.560042	8000.047610	12.849434	-0.058319	4.816042
284.493326	8000.054954	12.854439	-0.058307	4.816045
284.542446	7999.990674	12.859443	-0.058316	4.816026
284.501013	8000.072207	12.864448	-0.058308	4.816050
284.615832	8000.040110	12.869453	-0.058330	4.816040
284.729169	8000.057139	12.874458	-0.058351	4.816044
284.683821	8000.052048	12.879463	-0.058343	4.816043
284.596251	8000.059013	12.884467	-0.058326	4.816045
284.693754	8000.041560	12.889472	-0.058345	4.816040
284.669008	8000.003719	12.894477	-0.058340	4.816029
284.757675	8000.048082	12.899482	-0.058357	4.816041
284.751674	8000.051187	12.904487	-0.058356	4.816042
284.404324	8000.005343	12.909491	-0.058291	4.816031
284.555013	8000.031599	12.914496	-0.058319	4.816038
284.565064	8000.014694	12.919501	-0.058321	4.816033
284.567832	8000.005135	12.924506	-0.058322	4.816030
284.524617	8000.019318	12.929511	-0.058314	4.816034
284.499575	7999.961169	12.934515	-0.058309	4.816017
284.581798	8000.035334	12.939520	-0.058325	4.816039
284.519011	8000.012830	12.944525	-0.058313	4.816032
284.371458	8000.046486	12.949530	-0.058286	4.816043
284.551073	8000.034801	12.954535	-0.058319	4.816039
284.472665	8000.036589	12.959539	-0.058305	4.816040
284.561679	8000.033942	12.964544	-0.058321	4.816038
284.667378	8000.010227	12.969549	-0.058341	4.816031
284.567193	8000.013756	12.974554	-0.058323	4.816032
284.517175	8000.018198	12.979559	-0.058313	4.816034
284.650810	7999.931946	12.984563	-0.058338	4.816008
284.815095	7999.995850	12.989568	-0.058369	4.816026
284.722313	7999.935400	12.994573	-0.058352	4.816009
284.490112	8000.022014	12.999578	-0.058309	4.816035
284.683255	8000.037288	13.004583	-0.058345	4.816039
284.569960	7999.939067	13.009587	-0.058324	4.816010
284.679899	8000.021215	13.014592	-0.058344	4.816034
284.787412	7999.972957	13.019597	-0.058364	4.816019
284.827024	7999.998262	13.024602	-0.058372	4.816026
284.673952	8000.044641	13.029607	-0.058343	4.816041
284.606845	8000.013509	13.034611	-0.058331	4.816032
284.894547	8000.048669	13.039616	-0.058385	4.816041
284.621000	8000.024469	13.044621	-0.058334	4.816035
284.586026	8000.034527	13.049626	-0.058327	4.816038
284.745072	8000.023536	13.054631	-0.058357	4.816034
284.823837	8000.007880	13.059635	-0.058372	4.816029
284.521024	7999.999177	13.064640	-0.058315	4.816028
284.726996	7999.986902	13.069645	-0.058354	4.816024
284.740243	7999.999974	13.074650	-0.058356	4.816027
284.730623	8000.034001	13.079655	-0.058355	4.816037
284.557855	7999.996674	13.084659	-0.058323	4.816027
284.653273	8000.043297	13.089664	-0.058341	4.816040
284.580565	8000.010995	13.094669	-0.058327	4.816031
284.581480	7999.991786	13.099674	-0.058327	4.816026
284.759197	8000.005712	13.104679	-0.058361	4.816029
284.663885	8000.031769	13.109683	-0.058343	4.816037
284.730359	8000.076797	13.114688	-0.058355	4.816050
284.664769	8000.009363	13.119693	-0.058343	4.816030
284.765239	8000.012266	13.124698	-0.058362	4.816031
284.701520	8000.053858	13.129703	-0.058350	4.816043
284.732797	8000.027722	13.134707	-0.058356	4.816035
284.804605	8000.053613	13.139712	-0.058370	4.816043
284.843580	8000.058604	13.144717	-0.058377	4.816044
284.840952	8000.063908	13.149722	-0.058377	4.816045
284.831639	8000.032758	13.154727	-0.058375	4.816036
284.835062	8000.030692	13.159731	-0.058376	4.816036
284.617917	8000.067357	13.164736	-0.058335	4.816048
284.533861	8000.013478	13.169741	-0.058320	4.816032
284.610437	7999.994576	13.174746	-0.058334	4.816026
284.708905	8000.008129	13.179751	-0.058352	4.816030
284.596340	8000.023187	13.184755	-0.058332	4.816035
284.927895	8000.074104	13.189760	-0.058393	4.816048
284.740464	8000.026893	13.194765	-0.058359	4.816035
284.577295	8000.046374	13.199770	-0.058328	4.816042
284.678038	8000.061037	13.204775	-0.058347	4.816045
284.774594	7999.992277	13.209779	-0.058365	4.816025
284.779675	8000.010543	13.214784	-0.058366	4.816030
284.610507	8000.014955	13.219789	-0.058335	4.816032
285.048409	8000.003693	13.224794	-0.058416	4.816027
284.764263	8000.058373	13.229799	-0.058364	4.816044
284.607093	8000.010644	13.234803	-0.058334	4.816031
284.719318	8000.038338	13.239808	-0.058355	4.816039
284.736266	7999.974542	13.244813	-0.058359	4.816020
284.708047	8000.000751	13.249818	-0.058353	4.816028
284.782227	8000.044850	13.254823	-0.058367	4.816040
284.907536	7999.979818	13.259827	-0.058391	4.816020
284.788096	8000.012917	13.264832	-0.058369	4.816031
284.551288	8000.016099	13.269837	-0.058325	4.816033
284.749532	8000.018644	13.274842	-0.058362	4.816033
284.659560	8000.030908	13.279847	-0.058345	4.816037
284.678300	7999.978898	13.284851	-0.058349	4.816021
284.712096	7999.996617	13.289856	-0.058355	4.816026
284.881325	8000.010389	13.294861	-0.058387	4.816030
284.714556	8000.018050	13.299866	-0.058356	4.816033
284.743042	8000.018576	13.304871	-0.058361	4.816033
284.768732	8000.001955	13.309875	-0.058366	4.816028
284.978884	8000.030362	13.314880	-0.058405	4.816035
284.769597	7999.999850	13.319885	-0.058366	4.816027
284.895243	8000.003212	13.324890	-0.058390	4.816027
284.803979	8000.025069	13.329895	-0.058373	4.816034
284.663493	7999.986192	13.334899	-0.058347	4.816024
284.718998	7999.998964	13.339904	-0.058357	4.816027
284.811576	8000.026301	13.344909	-0.058374	4.816035
284.809999	8000.023075	13.349914	-0.058374	4.816034
284.874659	8000.040288	13.354919	-0.058386	4.816038
284.710666	8000.003120	13.359923	-0.058356	4.816028
284.837719	8000.053524	13.364928	-0.058380	4.816042
284.592621	7999.992442	13.369933	-0.058334	4.816026
284.742371	7999.980214	13.374938	-0.058362	4.816021
284.776642	8000.011833	13.379943	-0.058369	4.816030
284.601277	8000.005447	13.384947	-0.058336	4.816030
284.917039	8000.047529	13.389952	-0.058395	4.816040
284.877847	8000.035070	13.394957	-0.058388	4.816037
284.763097	8000.038335	13.399962	-0.058366	4.816038
284.952718	8000.049271	13.404967	-0.058402	4.816040
284.689904	8000.019924	13.409971	-0.058353	4.816033
284.941818	8000.070461	13.414976	-0.058400	4.816047
284.903943	8000.040930	13.419981	-0.058393	4.816038
284.882487	8000.013834	13.424986	-0.058389	4.816030
284.722918	8000.045134	13.429991	-0.058359	4.816040
284.633477	8000.032831	13.434995	-0.058343	4.816037
284.642263	8000.047959	13.440000	-0.058345	4.816042
284.724497	8000.051600	13.445005	-0.058360	4.816042
284.820083	8000.072580	13.450010	-0.058378	4.816048
284.876397	8000.049036	13.455015	-0.058388	4.816041
284.800961	8000.040193	13.460019	-0.058374	4.816039
284.949289	8000.052516	13.465024	-0.058402	4.816041
284.774679	8000.024772	13.470029	-0.058370	4.816034
284.797398	8000.063661	13.475034	-0.058374	4.816045
284.900510	8000.052722	13.480039	-0.058393	4.816042
284.766741	7999.973362	13.485043	-0.058368	4.816019
284.769183	8000.019362	13.490048	-0.058369	4.816033
284.825707	8000.018262	13.495053	-0.058380	4.816032
284.680359	7999.976090	13.500058	-0.058353	4.816020
284.595892	8000.017305	13.505063	-0.058337	4.816033
284.784230	7999.983339	13.510067	-0.058372	4.816022
284.836038	8000.034511	13.515072	-0.058382	4.816037
284.769036	8000.003382	13.520077	-0.058369	4.816028
284.711837	8000.023721	13.525082	-0.058359	4.816034
284.725731	8000.023982	13.530087	-0.058362	4.816034
284.565241	8000.018935	13.535091	-0.058332	4.816034
284.734272	8000.051937	13.540096	-0.058363	4.816042
284.956295	8000.042092	13.545101	-0.058405	4.816038
284.724247	8000.040017	13.550106	-0.058362	4.816039
284.890969	8000.066566	13.555111	-0.058393	4.816046
284.928200	8000.023440	13.560115	-0.058400	4.816033
284.951405	8000.043105	13.565120	-0.058404	4.816039
285.004025	8000.041933	13.570125	-0.058414	4.816038
285.006606	8000.011000	13.575130	-0.058415	4.816029
284.956786	8000.018651	13.580135	-0.058405	4.816031
284.872106	8000.008571	13.585139	-0.058390	4.816029
284.666176	7999.992012	13.590144	-0.058352	4.816025
284.739709	8000.019003	13.595149	-0.058365	4.816033
284.907318	8000.054116	13.600154	-0.058397	4.816042
284.893230	8000.062417	13.605159	-0.058394	4.816045
284.791788	8000.036003	13.610163	-0.058375	4.816037
285.017373	8000.056143	13.615168	-0.058417	4.816042
284.657606	8000.017552	13.620173	-0.058350	4.816033
284.623593	8000.029764	13.625178	-0.058344	4.816036
284.931714	8000.054610	13.630183	-0.058402	4.816042
284.786354	8000.008164	13.635187	-0.058375	4.816029
284.760729	8000.041900	13.640192	-0.058370	4.816039
284.837813	8000.049722	13.645197	-0.058384	4.816041
284.940278	7999.969315	13.650202	-0.058404	4.816017
284.759826	8000.008784	13.655207	-0.058370	4.816030
284.682762	7999.986020	13.660211	-0.058356	4.816023
285.018894	7999.971838	13.665216	-0.058418	4.816017
284.769354	7999.982268	13.670221	-0.058372	4.816022
284.889771	8000.034689	13.675226	-0.058395	4.816036
284.999291	8000.056992	13.680231	-0.058415	4.816042
284.931047	7999.984165	13.685235	-0.058402	4.816021
284.845263	7999.975134	13.690240	-0.058387	4.816019
284.831822	7999.993063	13.695245	-0.058384	4.816025
284.981756	7999.950919	13.700250	-0.058412	4.816011
285.009313	8000.006993	13.705255	-0.058417	4.816028
285.079036	7999.969802	13.710259	-0.058430	4.816016
285.076239	7999.948388	13.715264	-0.058430	4.816010
285.021644	7999.995489	13.720269	-0.058420	4.816024
284.996363	7999.998243	13.725274	-0.058415	4.816025
285.096822	8000.011833	13.730279	-0.058434	4.816029
285.074011	8000.019975	13.735283	-0.058430	4.816031
284.927069	8000.058985	13.740288	-0.058403	4.816043
284.951333	8000.000663	13.745293	-0.058407	4.816026
285.149356	8000.006410	13.750298	-0.058444	4.816027
285.016500	8000.062773	13.755303	-0.058420	4.816044
284.666736	8000.047872	13.760307	-0.058355	4.816041
284.839550	8000.055298	13.765312	-0.058387	4.816043
284.769832	8000.051901	13.770317	-0.058374	4.816042
284.671712	7999.974258	13.775322	-0.058356	4.816020
284.805842	8000.008762	13.780327	-0.058381	4.816029
284.781002	8000.020073	13.785331	-0.058376	4.816033
284.868228	8000.064410	13.790336	-0.058393	4.816045
284.845469	8000.035153	13.795341	-0.058388	4.816037
284.883296	8000.001656	13.800346	-0.058396	4.816027
284.984466	8000.036629	13.805351	-0.058415	4.816036
284.821978	7999.996283	13.810355	-0.058384	4.816025
284.950471	8000.031754	13.815360	-0.058408	4.816035
284.839085	8000.009434	13.820365	-0.058388	4.816029
284.794909	8000.028941	13.825370	-0.058380	4.816035
284.944696	8000.043428	13.830375	-0.058408	4.816039
285.005258	8000.003932	13.835379	-0.058419	4.816027
284.777548	7999.997663	13.840384	-0.058377	4.816026
284.895237	8000.013702	13.845389	-0.058399	4.816030
284.982294	8000.001403	13.850394	-0.058415	4.816026
285.027370	8000.044973	13.855399	-0.058423	4.816039
284.910438	7999.990496	13.860403	-0.058402	4.816023
284.860423	8000.038748	13.865408	-0.058392	4.816038
285.001891	7999.997518	13.870413	-0.058419	4.816025
284.877905	7999.945050	13.875418	-0.058396	4.816010
284.974827	7999.995974	13.880423	-0.058414	4.816025
285.128915	7999.994511	13.885427	-0.058443	4.816023
285.098682	8000.027095	13.890432	-0.058437	4.816033
284.982544	8000.022854	13.895437	-0.058416	4.816032
284.975585	8000.052656	13.900442	-0.058415	4.816041
285.032801	8000.048362	13.905447	-0.058425	4.816040
285.028444	8000.008754	13.910451	-0.058424	4.816028
285.064549	8000.062848	13.915456	-0.058431	4.816044
285.122045	8000.045736	13.920461	-0.058442	4.816038
284.975863	8000.009960	13.925466	-0.058415	4.816029
284.881366	8000.042444	13.930471	-0.058397	4.816039
284.927254	7999.996270	13.935475	-0.058406	4.816025
284.880005	8000.032819	13.940480	-0.058397	4.816036
284.913408	8000.058012	13.945485	-0.058404	4.816043
285.029020	8000.031272	13.950490	-0.058425	4.816035
285.051293	8000.070154	13.955495	-0.058430	4.816046
285.089071	8000.013146	13.960499	-0.058437	4.816029
285.168214	8000.031691	13.965504	-0.058451	4.816034
285.017507	8000.053536	13.970509	-0.058424	4.816041
285.190789	8000.039599	13.975514	-0.058456	4.816036
285.094952	8000.043207	13.980519	-0.058438	4.816038
285.063103	8000.006305	13.985523	-0.058432	4.816027
285.162316	8000.039106	13.990528	-0.058451	4.816036
285.172767	8000.035030	13.995533	-0.058453	4.816035
284.956333	8000.018279	14.000538	-0.058413	4.816031
285.051721	8000.021091	14.005543	-0.058430	4.816031
285.063957	8000.008499	14.010547	-0.058433	4.816028
285.201892	8000.025976	14.015552	-0.058459	4.816032
285.216954	8000.044424	14.020557	-0.058462	4.816037
285.154433	8000.035816	14.025562	-0.058450	4.816035
285.158432	8000.048720	14.030567	-0.058451	4.816039
284.997549	7999.991305	14.035571	-0.058421	4.816023
285.192129	8000.022635	14.040576	-0.058457	4.816031
285.040715	8000.022027	14.045581	-0.058429	4.816032
285.023566	8000.059123	14.050586	-0.058426	4.816043
284.999407	8000.062966	14.055591	-0.058422	4.816044
284.865986	8000.026354	14.060595	-0.058397	4.816034
284.838684	7999.985261	14.065600	-0.058392	4.816022
284.968588	7999.991906	14.070605	-0.058416	4.816023
285.050631	7999.930361	14.075610	-0.058431	4.816005
285.051360	8000.031896	14.080615	-0.058432	4.816035
285.138892	8000.026017	14.085619	-0.058448	4.816032
284.995348	7999.984946	14.090624	-0.058421	4.816021
284.990886	7999.997696	14.095629	-0.058421	4.816025
285.029828	8000.004824	14.100634	-0.058428	4.816027
285.091029	8000.021974	14.105639	-0.058440	4.816031
285.052197	7999.989219	14.110643	-0.058432	4.816022
285.105693	8000.037218	14.115648	-0.058442	4.816036
285.119677	8000.056715	14.120653	-0.058445	4.816041
284.950119	8000.045091	14.125658	-0.058414	4.816039
285.012788	8000.032347	14.130663	-0.058425	4.816035
285.022161	7999.991921	14.135667	-0.058427	4.816023
285.057050	8000.049198	14.140672	-0.058434	4.816040
284.986071	8000.054326	14.145677	-0.058421	4.816041
284.998850	8000.066322	14.150682	-0.058423	4.816045
285.261870	8000.094623	14.155687	-0.058472	4.816052
285.015033	8000.036713	14.160691	-0.058426	4.816036
285.063364	8000.040806	14.165696	-0.058435	4.816037
285.085147	8000.047622	14.170701	-0.058440	4.816039
285.133572	7999.980123	14.175706	-0.058449	4.816019
285.056212	8000.026810	14.180711	-0.058434	4.816033
285.007283	7999.989597	14.185715	-0.058425	4.816022
285.222778	7999.928342	14.190720	-0.058465	4.816003
284.980379	7999.979507	14.195725	-0.058420	4.816020
284.948923	8000.002452	14.200730	-0.058415	4.816026
285.251348	8000.060321	14.205735	-0.058471	4.816042
285.107141	8000.043815	14.210739	-0.058444	4.816038
285.068021	8000.040975	14.215744	-0.058437	4.816037
285.163255	8000.042715	14.220749	-0.058455	4.816037
285.126260	8000.001445	14.225754	-0.058448	4.816025
285.150375	8000.060663	14.230759	-0.058453	4.816042
285.076821	8000.030483	14.235763	-0.058439	4.816034
285.075854	8000.062530	14.240768	-0.058439	4.816043
284.829368	8000.031342	14.245773	-0.058393	4.816035
284.821149	8000.039749	14.250778	-0.058392	4.816038
285.202687	8000.069137	14.255783	-0.058463	4.816045
285.200503	8000.037048	14.260787	-0.058463	4.816035
285.150710	8000.052180	14.265792	-0.058453	4.816040
284.949437	7999.266356	14.270797	-0.058415	4.815811

285.132930	7995.975782	14.275802	-0.058448	4.814849
285.302846	7990.598669	14.280807	-0.058476	4.813276
285.064307	7983.887946	14.285811	-0.058427	4.811315
285.101988	7976.612965	14.290816	-0.058429	4.809187
285.103900	7969.040872	14.295821	-0.058425	4.806971
284.816865	7961.170934	14.300826	-0.058366	4.804668
284.863291	7953.410729	14.305831	-0.058370	4.802395
284.703229	7945.356767	14.310835	-0.058335	4.800035
284.702158	7937.484057	14.315840	-0.058330	4.797727
284.700248	7929.417235	14.320845	-0.058324	4.795360
284.652124	7921.387682	14.325850	-0.058310	4.793004
284.674797	7913.400445	14.330855	-0.058309	4.790658
284.539935	7905.429491	14.335859	-0.058279	4.788317
284.697040	7897.380002	14.340864	-0.058303	4.785950
284.588760	7889.464062	14.345869	-0.058278	4.783623
284.287747	7881.403746	14.350874	-0.058217	4.781253
284.533449	7873.483038	14.355879	-0.058258	4.778920
284.410515	7865.382578	14.360883	-0.058229	4.776535
284.279978	7857.396269	14.365888	-0.058200	4.774182
284.284548	7849.356627	14.370893	-0.058196	4.771812
284.337364	7841.357656	14.375898	-0.058200	4.769452
284.255998	7833.416794	14.380903	-0.058180	4.767109
284.040069	7825.336346	14.385907	-0.058135	4.764724
284.139628	7817.463007	14.390912	-0.058148	4.762398
284.205221	7809.369136	14.395917	-0.058155	4.760005
284.030096	7801.441828	14.400922	-0.058118	4.757662
284.017133	7793.441506	14.405927	-0.058110	4.755295
283.987360	7785.303660	14.410931	-0.058099	4.752887
283.856083	7777.266684	14.415936	-0.058070	4.750507
283.589109	7769.308992	14.420941	-0.058015	4.748150
283.610545	7761.315756	14.425946	-0.058014	4.745781
283.653086	7753.385702	14.430951	-0.058017	4.743429
283.618932	7745.369249	14.435955	-0.058005	4.741050
283.582236	7737.383094	14.440960	-0.057993	4.738679
283.540484	7729.374629	14.445965	-0.057980	4.736300
283.478767	7721.343729	14.450970	-0.057964	4.733914
283.440365	7713.276233	14.455975	-0.057951	4.731515
283.369290	7705.299575	14.460979	-0.057933	4.729143
283.575750	7697.325756	14.465984	-0.057966	4.726769
283.257132	7689.287420	14.470989	-0.057902	4.724376
283.201747	7681.311549	14.475994	-0.057886	4.722000
283.446447	7673.355350	14.480999	-0.057927	4.719627
283.255337	7665.362073	14.486003	-0.057886	4.717244
283.258261	7657.336121	14.491008	-0.057882	4.714849
283.183046	7649.307229	14.496013	-0.057862	4.712452
283.009483	7641.240781	14.501018	-0.057825	4.710043
283.034486	7633.366271	14.506023	-0.057825	4.707690
282.955271	7625.252576	14.511027	-0.057805	4.705264
282.915809	7617.315607	14.516032	-0.057792	4.702890
282.914524	7609.324602	14.521037	-0.057787	4.700498
282.902846	7601.286514	14.526042	-0.057779	4.698091
283.010686	7593.270213	14.531047	-0.057794	4.695689
282.790766	7585.296987	14.536051	-0.057748	4.693300
282.876177	7577.259551	14.541056	-0.057759	4.690889
282.863819	7569.310764	14.546061	-0.057752	4.688504
282.611327	7561.287310	14.551066	-0.057700	4.686095
282.637703	7553.319991	14.556071	-0.057699	4.683702
282.503501	7545.302641	14.561075	-0.057669	4.681293
282.430545	7537.316888	14.566080	-0.057650	4.678891
282.394890	7529.325146	14.571085	-0.057639	4.676487
282.354953	7521.217226	14.576090	-0.057626	4.674047
282.473753	7513.198510	14.581095	-0.057643	4.671632
282.284879	7505.179955	14.586099	-0.057603	4.669216
282.005392	7497.204438	14.591104	-0.057546	4.666812
282.195815	7489.231691	14.596109	-0.057576	4.664407
282.120413	7481.263594	14.601114	-0.057557	4.662002
282.241974	7473.234536	14.606119	-0.057574	4.659578
281.892483	7465.267128	14.611123	-0.057504	4.657171
281.968018	7457.266838	14.616128	-0.057513	4.654753
281.887919	7449.241049	14.621133	-0.057493	4.652326
281.804295	7441.166865	14.626138	-0.057472	4.649883
281.960329	7433.258840	14.631143	-0.057496	4.647489
281.780583	7425.177237	14.636147	-0.057458	4.645041
281.812476	7417.265594	14.641152	-0.057458	4.642643
281.894908	7409.218229	14.646157	-0.057469	4.640203
281.627334	7401.222182	14.651162	-0.057414	4.637778
281.770775	7393.236956	14.656167	-0.057435	4.635354
281.411108	7385.167933	14.661171	-0.057363	4.632903
281.747606	7377.219418	14.666176	-0.057421	4.630488
281.636232	7369.184362	14.671181	-0.057395	4.628045
281.319328	7361.135627	14.676186	-0.057331	4.625597
281.410381	7353.245068	14.681191	-0.057343	4.623196
281.486927	7345.195569	14.686195	-0.057352	4.620745
281.378021	7337.211418	14.691200	-0.057326	4.618312
281.470024	7329.199121	14.696205	-0.057338	4.615870
281.320552	7321.173250	14.701210	-0.057305	4.613422
281.008382	7313.179094	14.706215	-0.057242	4.610983
281.007285	7305.201943	14.711219	-0.057237	4.608548
281.086523	7297.191295	14.716224	-0.057246	4.606101
280.991981	7289.205162	14.721229	-0.057224	4.603660
280.927660	7281.154944	14.726234	-0.057206	4.601198
280.926748	7273.207027	14.731239	-0.057201	4.598767
280.775213	7265.164387	14.736243	-0.057168	4.596305
280.749102	7257.155681	14.741248	-0.057158	4.593852
280.914157	7249.117632	14.746253	-0.057183	4.591388
280.600063	7241.126762	14.751258	-0.057120	4.588938
280.568298	7233.139119	14.756263	-0.057109	4.586488
280.669755	7225.135330	14.761267	-0.057123	4.584031
280.603876	7217.141038	14.766272	-0.057105	4.581576
280.702689	7209.136659	14.771277	-0.057118	4.579116
280.265664	7201.170762	14.776282	-0.057032	4.576667
280.650947	7193.139061	14.781287	-0.057099	4.574197
280.439911	7185.172413	14.786291	-0.057054	4.571745
280.525597	7177.101111	14.791296	-0.057065	4.569259
280.335136	7169.132006	14.796301	-0.057024	4.566804
280.184907	7161.127692	14.801306	-0.056991	4.564336
280.363655	7153.189690	14.806311	-0.057019	4.561888
280.071238	7145.135793	14.811315	-0.056960	4.559402
280.232105	7137.194269	14.816320	-0.056985	4.556950
280.091990	7129.144743	14.821325	-0.056953	4.554463
280.034860	7121.061037	14.826330	-0.056938	4.551964
280.209121	7113.110168	14.831335	-0.056965	4.549505
280.187308	7105.115844	14.836339	-0.056956	4.547032
280.149524	7097.073529	14.841344	-0.056944	4.544541
280.133162	7089.168550	14.846349	-0.056935	4.542092
279.926898	7081.133724	14.851354	-0.056892	4.539602
279.981146	7073.159602	14.856359	-0.056897	4.537129
279.866370	7065.116168	14.861363	-0.056870	4.534633
279.678525	7057.110744	14.866368	-0.056830	4.532147
279.703990	7049.096663	14.871373	-0.056830	4.529658
279.519334	7041.123231	14.876378	-0.056790	4.527179
279.724574	7033.131055	14.881383	-0.056823	4.524694
279.411469	7025.127053	14.886387	-0.056760	4.522203
279.357452	7017.142126	14.891392	-0.056745	4.519717
279.360141	7009.198353	14.896397	-0.056740	4.517242
279.495455	7001.064844	14.901402	-0.056760	4.514708
279.428819	6993.032232	14.906407	-0.056743	4.512202
279.366213	6985.031097	14.911411	-0.056726	4.509706
279.121095	6977.041665	14.916416	-0.056675	4.507211
279.245769	6969.066164	14.921421	-0.056693	4.504720
279.161479	6961.092543	14.926426	-0.056672	4.502228
279.101974	6953.081276	14.931431	-0.056656	4.499722
278.927030	6945.087347	14.936435	-0.056619	4.497221
278.933827	6937.062635	14.941440	-0.056615	4.494708
279.056070	6929.093307	14.946445	-0.056632	4.492212
278.954824	6921.031606	14.951450	-0.056608	4.489685
278.846279	6913.093985	14.956455	-0.056583	4.487196
278.670154	6905.070879	14.961459	-0.056545	4.484678
278.715569	6897.113050	14.966464	-0.056548	4.482180
278.741798	6889.090268	14.971469	-0.056548	4.479660
278.671003	6881.056003	14.976474	-0.056530	4.477134
278.623650	6873.075712	14.981479	-0.056516	4.474624
278.501347	6865.027239	14.986483	-0.056488	4.472092
278.580556	6857.039912	14.991488	-0.056498	4.469577
278.364239	6849.040173	14.996493	-0.056452	4.467056
278.382251	6841.014945	15.001498	-0.056450	4.464527
278.332161	6833.068205	15.006503	-0.056436	4.462021
278.337711	6825.025473	15.011507	-0.056432	4.459483
278.313746	6817.032125	15.016512	-0.056422	4.456959
278.255746	6809.062465	15.021517	-0.056406	4.454441
278.101724	6800.996705	15.026522	-0.056373	4.451891
278.222718	6793.032202	15.031527	-0.056390	4.449372
278.222208	6785.014386	15.036531	-0.056385	4.446835
278.208047	6777.012157	15.041536	-0.056377	4.444301
277.984946	6769.101711	15.046541	-0.056330	4.441794
278.147775	6760.996218	15.051546	-0.056355	4.439226
278.061003	6753.043074	15.056551	-0.056334	4.436703
277.847696	6744.991827	15.061555	-0.056289	4.434147
277.761186	6736.979093	15.066560	-0.056268	4.431602
277.826457	6728.976912	15.071565	-0.056275	4.429060
277.580849	6720.940169	15.076570	-0.056224	4.426504
277.585746	6712.979424	15.081575	-0.056220	4.423972
277.746475	6705.017226	15.086579	-0.056245	4.421438
277.678456	6697.005812	15.091584	-0.056227	4.418886
277.661163	6688.992482	15.096589	-0.056219	4.416333
277.511827	6680.965097	15.101594	-0.056186	4.413773
277.680319	6672.985855	15.106599	-0.056212	4.411228
277.358510	6664.976183	15.111603	-0.056147	4.408670
277.307564	6656.959521	15.116608	-0.056132	4.406109
277.253103	6649.041357	15.121613	-0.056117	4.403579
277.143481	6640.999760	15.126618	-0.056092	4.401007
277.111170	6633.018319	15.131623	-0.056080	4.398453
277.125658	6624.996943	15.136627	-0.056078	4.395885
277.167266	6617.004192	15.141632	-0.056081	4.393325
277.115374	6608.958165	15.146637	-0.056066	4.390746
277.135145	6600.969277	15.151642	-0.056064	4.388184
277.244777	6592.942750	15.156647	-0.056080	4.385609
277.021126	6584.987598	15.161651	-0.056033	4.383054
276.699382	6577.019377	15.166656	-0.055968	4.380492
277.013567	6568.993836	15.171661	-0.056021	4.377914
276.893488	6560.960860	15.176666	-0.055994	4.375329
276.896401	6553.013010	15.181671	-0.055989	4.372772
276.660405	6544.954748	15.186675	-0.055940	4.370175
276.671980	6536.987116	15.191680	-0.055937	4.367608
276.471829	6529.001791	15.196685	-0.055895	4.365032
276.461194	6521.010129	15.201690	-0.055888	4.362454
276.536000	6513.015852	15.206695	-0.055896	4.359874
276.435389	6505.042062	15.211699	-0.055873	4.357298
276.413371	6496.986594	15.216704	-0.055863	4.354695
276.350045	6488.929011	15.221709	-0.055846	4.352089
276.257524	6480.919283	15.226714	-0.055824	4.349497
276.272804	6472.933523	15.231719	-0.055822	4.346911
276.206321	6464.909776	15.236723	-0.055804	4.344312
276.108810	6456.993535	15.241728	-0.055781	4.341745
276.250187	6449.021505	15.246733	-0.055802	4.339160
276.154365	6440.981955	15.251738	-0.055779	4.336551
276.285089	6432.999449	15.256743	-0.055798	4.333959
276.098349	6424.925330	15.261747	-0.055758	4.331335
276.008775	6416.956916	15.266752	-0.055737	4.328744
275.801172	6408.960260	15.271757	-0.055693	4.326141
275.867661	6400.969500	15.276762	-0.055700	4.323540
275.671164	6392.988110	15.281767	-0.055658	4.320939
275.698895	6384.978116	15.286771	-0.055658	4.318329
275.815420	6376.935646	15.291776	-0.055675	4.315707
275.812888	6368.986686	15.296781	-0.055669	4.313113
275.611100	6360.922598	15.301786	-0.055627	4.310479
275.749202	6352.958261	15.306791	-0.055647	4.307878
275.626146	6344.930021	15.311795	-0.055619	4.305253
275.611012	6336.958702	15.316800	-0.055611	4.302645
275.378050	6328.938989	15.321805	-0.055563	4.300019
275.554612	6320.944476	15.326810	-0.055591	4.297402
275.424957	6312.930386	15.331815	-0.055561	4.294775
275.251966	6304.925122	15.336819	-0.055524	4.292148
275.212600	6296.900781	15.341824	-0.055511	4.289515
275.159080	6288.923553	15.346829	-0.055496	4.286896
274.987737	6280.911281	15.351834	-0.055459	4.284263
275.207046	6272.963953	15.356839	-0.055495	4.281652
275.000613	6264.954826	15.361843	-0.055452	4.279016
274.835890	6256.937381	15.366848	-0.055416	4.276376
274.820084	6248.918458	15.371853	-0.055408	4.273735
274.776804	6240.867302	15.376858	-0.055394	4.271082
274.852274	6232.885413	15.381863	-0.055403	4.268451
274.700392	6224.889550	15.386867	-0.055370	4.265811
274.889398	6216.909913	15.391872	-0.055400	4.263178
274.700404	6208.910783	15.396877	-0.055360	4.260534
274.463846	6200.878272	15.401882	-0.055310	4.257877
274.422575	6192.904316	15.406887	-0.055298	4.255239
274.500238	6184.894499	15.411891	-0.055307	4.252589
274.469764	6176.889672	15.416896	-0.055296	4.249938
274.256073	6168.940872	15.421901	-0.055251	4.247302
274.289560	6160.880367	15.426906	-0.055252	4.244630
274.255095	6152.975387	15.431911	-0.055241	4.242007
274.140811	6144.926130	15.436915	-0.055214	4.239333
274.089206	6136.962967	15.441920	-0.055200	4.236687
274.118090	6128.922788	15.446925	-0.055200	4.234015
274.083239	6120.873496	15.451930	-0.055188	4.231337
274.226038	6112.914384	15.456935	-0.055210	4.228689
274.122849	6104.876218	15.461939	-0.055185	4.226011
274.040521	6096.955924	15.466944	-0.055165	4.223371
273.961542	6088.946937	15.471949	-0.055145	4.220699
273.781920	6080.972135	15.476954	-0.055107	4.218037
273.928241	6072.957520	15.481959	-0.055129	4.215362
273.797884	6064.971862	15.486963	-0.055099	4.212693
273.742977	6056.889229	15.491968	-0.055084	4.209990
273.740786	6048.939943	15.496973	-0.055078	4.207331
273.729846	6040.960521	15.501978	-0.055071	4.204660
273.659054	6032.977720	15.506983	-0.055053	4.201985
273.450744	6024.988339	15.511987	-0.055009	4.199305
273.376571	6016.946123	15.516992	-0.054990	4.196607
273.414765	6008.873148	15.521997	-0.054992	4.193898
273.326891	6000.793445	15.527002	-0.054971	4.191184
273.500941	5992.879978	15.532007	-0.054998	4.188526
273.287614	5984.886957	15.537011	-0.054953	4.185836
273.358955	5976.909762	15.542016	-0.054961	4.183153
273.298037	5968.935329	15.547021	-0.054945	4.180467
273.078608	5960.926598	15.552026	-0.054899	4.177767
273.239740	5952.916594	15.557031	-0.054924	4.175068
273.143040	5944.918110	15.562035	-0.054901	4.172369
273.014234	5936.871335	15.567040	-0.054871	4.169651
272.933224	5928.948433	15.572045	-0.054851	4.166974
272.767334	5920.890308	15.577050	-0.054815	4.164249
272.749446	5912.964636	15.582055	-0.054807	4.161568
272.785651	5904.943633	15.587059	-0.054808	4.158854
272.819637	5896.920559	15.592064	-0.054810	4.156137
273.004284	5888.883884	15.597069	-0.054839	4.153415
272.731177	5880.859487	15.602074	-0.054783	4.150691
272.746373	5872.905245	15.607079	-0.054780	4.147992
272.773567	5864.846398	15.612083	-0.054780	4.145256
272.466728	5856.931030	15.617088	-0.054718	4.142563
272.434200	5848.921565	15.622093	-0.054707	4.139839
272.524014	5840.891152	15.627098	-0.054719	4.137108
272.565343	5832.873197	15.632103	-0.054721	4.134379
272.327011	5824.875791	15.637107	-0.054672	4.131652
272.188425	5816.905902	15.642112	-0.054641	4.128933
272.112079	5808.900704	15.647117	-0.054621	4.126201
272.007038	5800.920150	15.652122	-0.054597	4.123476
272.134612	5792.924739	15.657127	-0.054615	4.120746
272.166382	5784.950804	15.662131	-0.054616	4.118021
271.999740	5776.912658	15.667136	-0.054580	4.115269
271.960499	5768.875340	15.672141	-0.054567	4.112518
271.934101	5760.858446	15.677146	-0.054557	4.109772
272.064150	5752.889453	15.682151	-0.054577	4.107042
271.720251	5744.888590	15.687155	-0.054507	4.104294
271.854633	5736.879141	15.692160	-0.054527	4.101547
272.115013	5728.926659	15.697165	-0.054571	4.098819
271.886079	5720.894169	15.702170	-0.054523	4.096056
271.824774	5712.948016	15.707175	-0.054506	4.093323
271.770919	5704.879039	15.712179	-0.054491	4.090545
271.664552	5696.918175	15.717184	-0.054466	4.087803
271.541473	5688.918964	15.722189	-0.054438	4.085045
271.514417	5680.963156	15.727194	-0.054428	4.082301
271.574960	5672.949635	15.732199	-0.054434	4.079537
271.453436	5664.970290	15.737203	-0.054406	4.076780
271.595232	5656.931023	15.742208	-0.054428	4.074004
271.528112	5648.946901	15.747213	-0.054410	4.071243
271.365917	5640.925974	15.752218	-0.054375	4.068466
271.185736	5632.923932	15.757223	-0.054336	4.065693
271.134753	5624.970031	15.762227	-0.054321	4.062936
271.281165	5616.921840	15.767232	-0.054344	4.060148
271.078675	5608.991202	15.772237	-0.054301	4.057394
270.952388	5600.905647	15.777242	-0.054272	4.054585
271.251258	5592.936958	15.782247	-0.054323	4.051821
271.067650	5584.948381	15.787251	-0.054283	4.049041
270.989784	5576.920672	15.792256	-0.054264	4.046247
270.909568	5568.965880	15.797261	-0.054244	4.043476
270.846207	5560.955861	15.802266	-0.054227	4.040685
270.910659	5552.978326	15.807271	-0.054234	4.037905
270.734164	5544.948337	15.812275	-0.054196	4.035101
270.634254	5536.826929	15.817280	-0.054172	4.032264
270.666919	5528.866502	15.822285	-0.054173	4.029484
270.599322	5520.891704	15.827290	-0.054155	4.026695
270.607540	5512.917457	15.832295	-0.054152	4.023906
270.471249	5504.928174	15.837299	-0.054121	4.021107
270.340445	5496.950519	15.842304	-0.054092	4.018310
270.521311	5488.931208	15.847309	-0.054120	4.015501
270.518747	5480.916489	15.852314	-0.054114	4.012690
270.299329	5472.919501	15.857319	-0.054068	4.009879
270.258195	5464.936416	15.862323	-0.054056	4.007074
270.277194	5456.883510	15.867328	-0.054054	4.004243
270.373417	5448.945556	15.872333	-0.054067	4.001452
270.180782	5440.946118	15.877338	-0.054026	3.998633
270.157560	5432.950187	15.882343	-0.054016	3.995816
270.268060	5424.892854	15.887347	-0.054032	3.992977
269.920611	5416.873268	15.892352	-0.053962	3.990142
269.953903	5408.921044	15.897357	-0.053963	3.987335
269.942215	5400.863380	15.902362	-0.053956	3.984488
269.875831	5392.938438	15.907367	-0.053938	3.981685
269.727537	5384.950520	15.912371	-0.053906	3.978857
269.768708	5376.925285	15.917376	-0.053908	3.976016
269.839284	5368.949344	15.922381	-0.053916	3.973191
269.689026	5360.886282	15.927386	-0.053883	3.970330
269.752323	5352.961674	15.932391	-0.053890	3.967519
269.757023	5344.937285	15.937395	-0.053885	3.964670
269.431900	5337.006139	15.942400	-0.053820	3.961846
269.573402	5329.036025	15.947405	-0.053841	3.959015
269.429108	5320.990336	15.952410	-0.053809	3.956149
269.436695	5312.949477	15.957415	-0.053805	3.953286
269.475452	5304.910335	15.962419	-0.053807	3.950422
269.321343	5296.951871	15.967424	-0.053774	3.947581
269.244433	5288.995502	15.972429	-0.053754	3.944741
268.956635	5280.999141	15.977434	-0.053695	3.941880
269.076813	5272.998574	15.982439	-0.053713	3.939023
269.024921	5265.005149	15.987443	-0.053698	3.936163
268.886780	5256.975556	15.992448	-0.053667	3.933287
268.937605	5248.976627	15.997453	-0.053671	3.930423
268.776119	5241.014852	16.002458	-0.053636	3.927566
268.914075	5233.002398	16.007463	-0.053657	3.924694
268.788397	5225.027082	16.012467	-0.053628	3.921829
268.777838	5217.013700	16.017472	-0.053621	3.918950
268.977586	5208.988765	16.022477	-0.053653	3.916069
268.725121	5200.957640	16.027482	-0.053601	3.913175
268.743183	5192.977894	16.032487	-0.053599	3.910303
268.768966	5185.030473	16.037491	-0.053599	3.907440
268.567364	5176.995676	16.042496	-0.053556	3.904539
268.578557	5169.017514	16.047501	-0.053553	3.901661
268.297386	5161.006604	16.052506	-0.053496	3.898763
268.268741	5153.040635	16.057511	-0.053485	3.895884
268.221728	5145.000398	16.062515	-0.053471	3.892975
268.148384	5136.968422	16.067520	-0.053453	3.890067
268.141312	5129.036421	16.072525	-0.053446	3.887194
268.013918	5120.997738	16.077530	-0.053417	3.884278
268.220941	5113.027679	16.082535	-0.053451	3.881391
268.134234	5105.041059	16.087539	-0.053430	3.878491
268.092489	5097.022863	16.092544	-0.053417	3.875577
267.998809	5088.790268	16.097549	-0.053394	3.872583
267.827954	5080.810943	16.102554	-0.053357	3.869676
267.803804	5072.907878	16.107559	-0.053347	3.866799
267.669322	5064.948092	16.112563	-0.053317	3.863896
267.677886	5056.957574	16.117568	-0.053314	3.860982
267.724626	5049.018072	16.122573	-0.053317	3.858086
267.744623	5040.994524	16.127578	-0.053316	3.855156
267.590483	5033.022385	16.132583	-0.053282	3.852240
267.463397	5025.007954	16.137587	-0.053253	3.849306
267.312880	5017.003533	16.142592	-0.053220	3.846373
267.307258	5009.039089	16.147597	-0.053214	3.843456
267.273481	5001.049900	16.152602	-0.053203	3.840526
267.175241	4993.079746	16.157607	-0.053179	3.837600
267.095246	4985.046706	16.162611	-0.053159	3.834649
267.034291	4977.052807	16.167616	-0.053143	3.831711
267.146215	4969.037600	16.172621	-0.053158	3.828766
266.917942	4961.040789	16.177626	-0.053111	3.825819
267.165995	4953.054827	16.182631	-0.053152	3.822883
267.144746	4945.071460	16.187635	-0.053143	3.819940
266.930032	4937.107748	16.192640	-0.053098	3.816998
266.884868	4929.093302	16.197645	-0.053084	3.814039
266.956190	4921.069172	16.202650	-0.053092	3.811076
267.114280	4913.074995	16.207655	-0.053117	3.808124
266.831736	4905.104646	16.212659	-0.053059	3.805169
266.728912	4897.126900	16.217664	-0.053035	3.802212
266.825183	4889.115276	16.222669	-0.053047	3.799246
266.683679	4881.103460	16.227674	-0.053016	3.796271
266.694550	4873.074836	16.232679	-0.053013	3.793292
266.440933	4865.043591	16.237683	-0.052960	3.790303
266.491870	4857.079879	16.242688	-0.052965	3.787344
266.483284	4849.109095	16.247693	-0.052958	3.784378
266.245446	4841.112820	16.252698	-0.052909	3.781396
266.294147	4833.114395	16.257703	-0.052913	3.778416
266.229720	4825.094664	16.262707	-0.052895	3.775424
266.222165	4817.046166	16.267712	-0.052889	3.772420
266.279932	4809.114653	16.272717	-0.052895	3.769459
266.168618	4801.092622	16.277722	-0.052869	3.766458
266.016559	4793.147058	16.282727	-0.052835	3.763482
266.142706	4785.125226	16.287731	-0.052854	3.760481
266.067380	4777.142759	16.292736	-0.052835	3.757489
265.969806	4769.154725	16.297741	-0.052811	3.754491
265.932723	4761.077139	16.302746	-0.052799	3.751458
265.996941	4753.076356	16.307751	-0.052806	3.748455
265.790267	4745.083621	16.312755	-0.052762	3.745445
265.688401	4737.116679	16.317760	-0.052738	3.742446
265.882830	4729.144533	16.322765	-0.052769	3.739449
265.686520	4721.139931	16.327770	-0.052728	3.736428
265.508424	4713.133318	16.332775	-0.052689	3.733404
265.573406	4705.109047	16.337779	-0.052696	3.730377
265.622024	4697.112117	16.342784	-0.052700	3.727357
265.652252	4689.121978	16.347789	-0.052701	3.724338
265.441026	4681.179881	16.352794	-0.052656	3.721328
265.546132	4673.211181	16.357799	-0.052671	3.718313
265.285471	4665.193802	16.362803	-0.052617	3.715268
265.204830	4657.098470	16.367808	-0.052597	3.712196
265.249396	4649.121123	16.372813	-0.052600	3.709169
265.034464	4641.107690	16.377818	-0.052555	3.706119
265.198914	4633.182548	16.382823	-0.052581	3.703110
265.301255	4625.173459	16.387827	-0.052594	3.700065
265.215115	4617.204367	16.392832	-0.052573	3.697028
264.903170	4609.243353	16.397837	-0.052510	3.693985
264.847366	4601.184914	16.402842	-0.052495	3.690910
264.926593	4593.229889	16.407847	-0.052504	3.687875
264.780217	4585.202985	16.412851	-0.052472	3.684804
264.539731	4577.282022	16.417856	-0.052422	3.681769
264.664680	4569.250792	16.422861	-0.052440	3.678698
264.821287	4561.246132	16.427866	-0.052464	3.675636
264.572019	4553.252061	16.432871	-0.052413	3.672564
264.624617	4545.210664	16.437875	-0.052417	3.669480
264.575701	4537.205500	16.442880	-0.052403	3.666405
264.629558	4529.238402	16.447885	-0.052408	3.663344
264.520910	4521.225512	16.452890	-0.052383	3.660259
264.426960	4513.294642	16.457895	-0.052360	3.657203
264.235368	4505.266860	16.462899	-0.052319	3.654105
264.316877	4497.236492	16.467904	-0.052329	3.651010
264.399793	4489.267785	16.472909	-0.052340	3.647936
264.263303	4481.215604	16.477914	-0.052309	3.644822
264.157224	4473.307133	16.482919	-0.052284	3.641762
264.094391	4465.295967	16.487923	-0.052267	3.638660
264.104350	4457.281054	16.492928	-0.052264	3.635556
264.001541	4449.276685	16.497933	-0.052240	3.632450
263.644828	4441.246786	16.502938	-0.052168	3.629326
263.892137	4433.233792	16.507943	-0.052209	3.626221
263.872712	4425.298177	16.512947	-0.052200	3.623136
263.712018	4417.290066	16.517952	-0.052165	3.620017
263.770204	4409.358699	16.522957	-0.052171	3.616931
263.887580	4401.305013	16.527962	-0.052188	3.613796
263.819302	4393.315251	16.532967	-0.052170	3.610679
263.705175	4385.333240	16.537971	-0.052144	3.607560
263.619999	4377.305828	16.542976	-0.052123	3.604422
263.544723	4369.369356	16.547981	-0.052103	3.601317
263.281775	4361.391623	16.552986	-0.052049	3.598187
263.428540	4353.369622	16.557991	-0.052072	3.595049
263.364694	4345.378281	16.562995	-0.052055	3.591915
263.199595	4337.363781	16.568000	-0.052019	3.588766
263.297817	4329.386062	16.573005	-0.052032	3.585636
263.230081	4321.383489	16.578010	-0.052014	3.582488
263.181921	4313.401651	16.583015	-0.052000	3.579347
263.091592	4305.424335	16.588019	-0.051978	3.576204
263.087660	4297.403499	16.593024	-0.051972	3.573042
263.063726	4289.386468	16.598029	-0.051963	3.569880
263.083009	4281.424802	16.603034	-0.051961	3.566737
262.879347	4273.454786	16.608039	-0.051918	3.563582
262.959511	4265.449119	16.613043	-0.051928	3.560418
262.688255	4257.487291	16.618048	-0.051872	3.557259
262.764643	4249.422879	16.623053	-0.051881	3.554066
262.634906	4241.342290	16.628058	-0.051852	3.550858
262.709116	4233.368812	16.633063	-0.051861	3.547695
262.705261	4225.393264	16.638067	-0.051855	3.544526
262.493363	4217.441068	16.643072	-0.051810	3.541358
262.422427	4209.476984	16.648077	-0.051792	3.538187
262.362268	4201.435451	16.653082	-0.051776	3.534982
262.406380	4193.438065	16.658087	-0.051779	3.531794
262.351238	4185.430297	16.663091	-0.051763	3.528597
262.265397	4177.443062	16.668096	-0.051742	3.525404
262.400464	4169.492521	16.673101	-0.051762	3.522230
261.995051	4161.514261	16.678106	-0.051682	3.519025
262.065836	4153.523768	16.683111	-0.051690	3.515827
261.877864	4145.509562	16.688115	-0.051650	3.512608
261.979838	4137.485393	16.693120	-0.051663	3.509392
262.111035	4129.495059	16.698125	-0.051683	3.506187
261.895049	4121.520678	16.703130	-0.051637	3.502974
261.981988	4113.518077	16.708135	-0.051648	3.499757
261.916614	4105.559305	16.713139	-0.051631	3.496550
261.732336	4097.545041	16.718144	-0.051592	3.493314
261.716906	4089.538394	16.723149	-0.051584	3.490083
261.665172	4081.559759	16.728154	-0.051569	3.486859
261.739730	4073.576406	16.733159	-0.051578	3.483634
261.532156	4065.616213	16.738163	-0.051534	3.480407
261.431915	4057.626616	16.743168	-0.051510	3.477168
261.616118	4049.612249	16.748173	-0.051539	3.473925
261.344772	4041.578723	16.753178	-0.051484	3.470657
261.355479	4033.574512	16.758183	-0.051481	3.467407
261.188982	4025.614806	16.763187	-0.051444	3.464166
261.294709	4017.611206	16.768192	-0.051459	3.460913
261.175290	4009.674301	16.773197	-0.051432	3.457677
261.062349	4001.637968	16.778202	-0.051406	3.454397
261.026349	3993.639908	16.783207	-0.051394	3.451132
260.962596	3985.674574	16.788211	-0.051377	3.447877
260.989240	3977.615677	16.793216	-0.051377	3.444583
261.037501	3969.683236	16.798221	-0.051380	3.441339
260.929478	3961.656542	16.803226	-0.051355	3.438048
260.826521	3953.686655	16.808231	-0.051331	3.434777
260.934514	3945.634373	16.813235	-0.051346	3.431476
260.743460	3937.662629	16.818240	-0.051305	3.428195
260.581635	3929.670433	16.823245	-0.051270	3.424903
260.518093	3921.727288	16.828250	-0.051253	3.421632
260.613315	3913.708377	16.833255	-0.051266	3.418332
260.453462	3905.729378	16.838259	-0.051231	3.415036
260.401862	3897.719804	16.843264	-0.051216	3.411729
260.307218	3889.732891	16.848269	-0.051193	3.408426
260.492725	3881.705047	16.853274	-0.051223	3.405112
260.487714	3873.790363	16.858279	-0.051217	3.401835
260.336120	3865.809588	16.863283	-0.051183	3.398523
260.179158	3857.805516	16.868288	-0.051149	3.395198
260.162299	3849.757884	16.873293	-0.051141	3.391856
260.002766	3841.739844	16.878298	-0.051106	3.388518
259.976805	3833.755384	16.883303	-0.051096	3.385196
259.981143	3825.804719	16.888307	-0.051092	3.381885
259.938460	3817.799908	16.893312	-0.051078	3.378547
259.915320	3809.832800	16.898317	-0.051069	3.375222
259.661353	3801.819047	16.903322	-0.051017	3.371867
259.559917	3793.834099	16.908327	-0.050993	3.368525
259.699355	3785.824797	16.913331	-0.051013	3.365178
259.738170	3777.858760	16.918336	-0.051016	3.361842
259.801170	3769.876976	16.923341	-0.051022	3.358498
259.534223	3761.881442	16.928346	-0.050967	3.355132
259.669958	3753.852220	16.933351	-0.050987	3.351764
259.548900	3745.889361	16.938355	-0.050960	3.348410
259.414463	3737.871947	16.943360	-0.050930	3.345030
259.641219	3729.922700	16.948365	-0.050967	3.341688
259.314219	3721.936596	16.953370	-0.050901	3.338308
259.210199	3713.956464	16.958375	-0.050876	3.334934
259.217234	3705.946051	16.963379	-0.050872	3.331548
259.234847	3697.907466	16.968384	-0.050871	3.328147
259.324631	3689.930484	16.973389	-0.050882	3.324772
259.253383	3681.988120	16.978394	-0.050864	3.321402
259.260460	3673.995546	16.983399	-0.050860	3.318009
259.125203	3666.010396	16.988403	-0.050830	3.314612
258.720654	3657.994785	16.993408	-0.050749	3.311188
258.848378	3650.008985	16.998413	-0.050768	3.307792
258.776105	3641.985269	17.003418	-0.050749	3.304370
258.591876	3634.054402	17.008423	-0.050710	3.300980
258.673123	3626.068804	17.013427	-0.050720	3.297572
258.682416	3618.056939	17.018432	-0.050717	3.294147
258.725357	3610.035100	17.023437	-0.050719	3.290716
258.595340	3602.049416	17.028442	-0.050690	3.287290
258.546186	3594.082360	17.033447	-0.050676	3.283871
258.497309	3586.103252	17.038451	-0.050662	3.280444
258.428010	3578.120548	17.043456	-0.050644	3.277011
258.382074	3570.124561	17.048461	-0.050630	3.273569
258.350964	3562.099446	17.053466	-0.050619	3.270112
258.291172	3554.132474	17.058471	-0.050603	3.266675
258.201174	3546.150625	17.063475	-0.050581	3.263226
258.183928	3538.123713	17.068480	-0.050572	3.259758
258.094202	3530.191310	17.073485	-0.050551	3.256324
257.849623	3522.152424	17.078490	-0.050500	3.252834
258.099067	3514.180850	17.083495	-0.050541	3.249388
257.972162	3506.204585	17.088499	-0.050513	3.245923
257.897774	3498.201197	17.093504	-0.050494	3.242444
258.041707	3490.210059	17.098509	-0.050515	3.238975
258.088816	3482.224861	17.103514	-0.050519	3.235501
257.723698	3474.201048	17.108519	-0.050446	3.231990
257.797981	3466.184127	17.113523	-0.050455	3.228496
257.822808	3458.180435	17.118528	-0.050454	3.225002
257.553162	3450.259864	17.123533	-0.050399	3.221528
257.353996	3442.277957	17.128538	-0.050357	3.218027
257.483904	3434.289105	17.133543	-0.050376	3.214532
257.451586	3426.272107	17.138547	-0.050364	3.211014
257.273125	3418.287549	17.143552	-0.050326	3.207501
257.303665	3410.305704	17.148557	-0.050327	3.203994
257.260616	3402.330998	17.153562	-0.050314	3.200483
257.188331	3394.385530	17.158567	-0.050295	3.196980
257.248045	3386.354273	17.163571	-0.050301	3.193440
257.038289	3378.358805	17.168576	-0.050257	3.189902
257.092354	3370.407307	17.173581	-0.050262	3.186389
256.975724	3362.391920	17.178586	-0.050235	3.182838
257.154168	3354.383510	17.183591	-0.050263	3.179298
257.236163	3346.416353	17.188595	-0.050273	3.175768
256.991259	3338.410553	17.193600	-0.050222	3.172203
257.073775	3330.436568	17.198605	-0.050233	3.168663
256.993217	3322.429609	17.203610	-0.050213	3.165096
256.805324	3314.505081	17.208615	-0.050172	3.161558
256.701645	3306.524732	17.213619	-0.050148	3.157995
256.745430	3298.486092	17.218624	-0.050151	3.154407
256.815748	3290.456802	17.223629	-0.050159	3.150822
256.632034	3282.491233	17.228634	-0.050120	3.147249
256.556691	3274.506167	17.233639	-0.050101	3.143668
256.466526	3266.534464	17.238643	-0.050079	3.140089
256.233666	3258.583038	17.243648	-0.050030	3.136508
256.286534	3250.584428	17.248653	-0.050035	3.132915
256.412969	3242.547556	17.253658	-0.050053	3.129303
256.300223	3234.605002	17.258663	-0.050027	3.125720
256.148344	3226.638113	17.263667	-0.049994	3.122119
256.095758	3218.648604	17.268672	-0.049979	3.118509
256.203948	3210.637324	17.273677	-0.049994	3.114891
255.988512	3202.640426	17.278682	-0.049949	3.111261
256.075125	3194.656084	17.283687	-0.049960	3.107647
255.851317	3186.700811	17.288691	-0.049913	3.104027
255.868614	3178.715148	17.293696	-0.049911	3.100400
255.926383	3170.730672	17.298701	-0.049917	3.096772
255.877092	3162.720310	17.303706	-0.049902	3.093122
255.661131	3154.723789	17.308711	-0.049857	3.089467
255.594464	3146.752637	17.313715	-0.049839	3.085826
255.532283	3138.772044	17.318720	-0.049823	3.082176
255.653358	3130.814544	17.323725	-0.049840	3.078541
255.349669	3122.815218	17.328730	-0.049779	3.074863
255.255556	3114.743890	17.333735	-0.049756	3.071157
255.404592	3106.754233	17.338739	-0.049778	3.067496
255.234736	3098.766345	17.343744	-0.049742	3.063816
255.275015	3090.808816	17.348749	-0.049744	3.060155
255.422703	3082.860009	17.353754	-0.049767	3.056499
255.275827	3074.870889	17.358759	-0.049734	3.052807
255.082270	3066.888179	17.363763	-0.049693	3.049110
255.033706	3058.886908	17.368768	-0.049679	3.045407
255.099858	3050.955051	17.373773	-0.049686	3.041738
254.966022	3042.953013	17.378778	-0.049656	3.038022
254.813678	3034.984253	17.383783	-0.049622	3.034316
254.810529	3026.956876	17.388787	-0.049617	3.030585
254.789111	3018.976815	17.393792	-0.049608	3.026871
254.780568	3011.001210	17.398797	-0.049601	3.023154
254.623696	3003.038770	17.403802	-0.049567	3.019433
254.471123	2995.060398	17.408807	-0.049533	3.015699
254.555129	2987.049995	17.413811	-0.049544	3.011957
254.525716	2979.034019	17.418816	-0.049533	3.008203
254.497816	2971.064515	17.423821	-0.049523	3.004465
254.362538	2963.122839	17.428826	-0.049492	3.000731
254.344035	2955.148326	17.433831	-0.049484	2.996983
254.505536	2947.130396	17.438835	-0.049509	2.993218
254.458284	2939.106051	17.443840	-0.049495	2.989435
254.411026	2931.136203	17.448845	-0.049481	2.985673
254.011576	2923.205734	17.453850	-0.049401	2.981907
253.952689	2915.234908	17.458855	-0.049385	2.978135
253.968739	2907.238589	17.463859	-0.049383	2.974349
253.888140	2899.213366	17.468864	-0.049363	2.970540
253.916439	2891.250630	17.473869	-0.049363	2.966761
253.701285	2883.278057	17.478874	-0.049318	2.962960
253.701771	2875.312442	17.483879	-0.049313	2.959169
253.825249	2867.326845	17.488883	-0.049331	2.955369
253.695087	2859.308053	17.493888	-0.049302	2.951536
253.623481	2851.333284	17.498893	-0.049283	2.947722
253.682362	2843.345697	17.503898	-0.049289	2.943903
253.448131	2835.381825	17.508903	-0.049240	2.940076
253.415882	2827.427434	17.513907	-0.049229	2.936259
253.282840	2819.407924	17.518912	-0.049199	2.932400
253.341983	2811.435286	17.523917	-0.049205	2.928569
253.238857	2803.446626	17.528922	-0.049181	2.924716
253.432166	2795.472516	17.533927	-0.049212	2.920881
253.391684	2787.520052	17.538931	-0.049199	2.917039
253.364581	2779.457892	17.543936	-0.049189	2.913140
253.311492	2771.462228	17.548941	-0.049174	2.909266
253.262120	2763.489706	17.553946	-0.049160	2.905398
253.126848	2755.538545	17.558951	-0.049129	2.901531
252.988274	2747.595210	17.563955	-0.049098	2.897663
252.736100	2739.600721	17.568960	-0.049046	2.893758
252.655348	2731.611678	17.573965	-0.049026	2.889860
252.664918	2723.633057	17.578970	-0.049023	2.885967
252.589232	2715.663792	17.583975	-0.049004	2.882068
252.678323	2707.682601	17.588979	-0.049015	2.878167
252.556989	2699.678914	17.593984	-0.048987	2.874238
252.499223	2691.717304	17.598989	-0.048972	2.870328
252.528001	2683.707395	17.603994	-0.048972	2.866394
252.474515	2675.727806	17.608999	-0.048957	2.862465
252.487066	2667.758141	17.614003	-0.048954	2.858538
252.256887	2659.796923	17.619008	-0.048906	2.854597
252.504502	2651.793779	17.624013	-0.048947	2.850657
252.354221	2643.826797	17.629018	-0.048914	2.846707
252.165873	2635.882802	17.634023	-0.048874	2.842760
252.276033	2627.914975	17.639027	-0.048889	2.838813
252.034750	2619.922575	17.644032	-0.048839	2.834828
252.100868	2611.925522	17.649037	-0.048846	2.830853
251.900839	2603.942950	17.654042	-0.048804	2.826864
251.975269	2595.958681	17.659047	-0.048813	2.822885
251.774515	2588.011352	17.664051	-0.048770	2.818902
251.660768	2580.018053	17.669056	-0.048744	2.814896
251.913466	2572.014861	17.674061	-0.048786	2.810900
251.722513	2564.043856	17.679066	-0.048745	2.806890
251.721544	2556.067530	17.684071	-0.048740	2.802881
251.670777	2548.119492	17.689075	-0.048725	2.798878
251.478953	2540.135320	17.694080	-0.048684	2.794844
251.695662	2532.115080	17.699085	-0.048720	2.790808
251.395989	2524.173342	17.704090	-0.048659	2.786777
251.554481	2516.184113	17.709095	-0.048683	2.782742
251.551558	2508.219540	17.714099	-0.048677	2.778705
251.176872	2500.272193	17.719104	-0.048603	2.774649
251.190679	2492.265748	17.724109	-0.048600	2.770579
251.066210	2484.304314	17.729114	-0.048572	2.766518
250.850621	2476.351190	17.734119	-0.048527	2.762450
250.909856	2468.374744	17.739123	-0.048532	2.758381
250.948075	2460.347219	17.744128	-0.048534	2.754278
250.889036	2452.299785	17.749133	-0.048518	2.750153
250.649943	2444.362836	17.754138	-0.048469	2.746067
250.890394	2436.370510	17.759143	-0.048508	2.741976
251.008989	2428.403115	17.764147	-0.048525	2.737885
250.708387	2420.449791	17.769152	-0.048464	2.733768
250.777138	2412.456501	17.774157	-0.048472	2.729648
250.744046	2404.488502	17.779162	-0.048461	2.725528
250.389723	2396.576681	17.784167	-0.048390	2.721412
250.459877	2388.609167	17.789171	-0.048398	2.717286
250.265326	2380.603477	17.794176	-0.048356	2.713118
250.383564	2372.610729	17.799181	-0.048373	2.708969
250.282201	2364.634796	17.804186	-0.048349	2.704809
250.348383	2356.664320	17.809191	-0.048356	2.700657
250.493738	2348.708529	17.814195	-0.048378	2.696510
250.257956	2340.723538	17.819200	-0.048329	2.692318
250.150530	2332.758324	17.824205	-0.048304	2.688137
250.060683	2324.785611	17.829210	-0.048282	2.683948
250.263637	2316.795453	17.834215	-0.048315	2.679761
250.228995	2308.873599	17.839219	-0.048303	2.675588
250.105812	2300.851763	17.844224	-0.048275	2.671351
250.123277	2292.870586	17.849229	-0.048273	2.667137
249.963803	2284.910493	17.854234	-0.048239	2.662916
249.645820	2276.982955	17.859239	-0.048174	2.658696
249.731072	2269.005601	17.864243	-0.048185	2.654468
249.769279	2260.966518	17.869248	-0.048187	2.650198
249.559239	2253.044797	17.874253	-0.048143	2.645968
249.507510	2245.079650	17.879258	-0.048128	2.641717
249.639037	2237.092351	17.884263	-0.048148	2.637460
249.490262	2229.137082	17.889267	-0.048115	2.633195
249.332657	2221.144345	17.894272	-0.048080	2.628902
249.358347	2213.170972	17.899277	-0.048080	2.624625
249.298356	2205.201116	17.904282	-0.048064	2.620337
249.364824	2197.238869	17.909287	-0.048071	2.616054
249.278709	2189.270014	17.914291	-0.048050	2.611751
249.026192	2181.306069	17.919296	-0.047998	2.607432
249.076721	2173.354206	17.924301	-0.048002	2.603133
248.988623	2165.383454	17.929306	-0.047980	2.598807
248.947770	2157.394863	17.934311	-0.047968	2.594467
248.870361	2149.251558	17.939315	-0.047948	2.590033
248.849955	2141.282045	17.944320	-0.047939	2.585691
248.938176	2133.377237	17.949325	-0.047951	2.581383
248.757596	2125.436744	17.954330	-0.047912	2.577031
248.570732	2117.502580	17.959335	-0.047872	2.572674
248.627401	2109.525506	17.964339	-0.047877	2.568303
248.499082	2101.563944	17.969344	-0.047848	2.563921
248.590680	2093.607641	17.974349	-0.047860	2.559549
248.379894	2085.659445	17.979354	-0.047816	2.555152
248.631759	2077.639767	17.984359	-0.047858	2.550742
248.316992	2069.713959	17.989363	-0.047794	2.546335
248.047670	2061.768432	17.994368	-0.047739	2.541914
248.105006	2053.802734	17.999373	-0.047744	2.537496
248.057322	2045.819902	18.004378	-0.047730	2.533054
248.133816	2037.837247	18.009383	-0.047740	2.528612
248.137034	2029.877069	18.014387	-0.047735	2.524171
248.041525	2021.935132	18.019392	-0.047712	2.519724
248.141723	2013.976666	18.024397	-0.047726	2.515275
247.935561	2005.972484	18.029402	-0.047682	2.510770
247.849228	1998.006268	18.034407	-0.047661	2.506287
247.674973	1990.070081	18.039411	-0.047624	2.501806
247.424850	1982.118157	18.044416	-0.047572	2.497303
247.574353	1974.137509	18.049421	-0.047595	2.492804
247.415162	1966.163893	18.054426	-0.047560	2.488279
247.259136	1958.214090	18.059431	-0.047526	2.483759
247.469487	1950.251188	18.064435	-0.047560	2.479251
247.579945	1942.273111	18.069440	-0.047575	2.474718
247.488246	1934.298077	18.074445	-0.047553	2.470164
247.343096	1926.339837	18.079450	-0.047521	2.465607
247.283583	1918.383062	18.084455	-0.047505	2.461049
247.190045	1910.454472	18.089459	-0.047482	2.456496
246.996648	1902.485806	18.094464	-0.047441	2.451903
247.026878	1894.502660	18.099469	-0.047442	2.447311
246.879406	1886.563972	18.104474	-0.047409	2.442722
246.897231	1878.607262	18.109479	-0.047407	2.438127
246.745281	1870.653083	18.114483	-0.047374	2.433512
246.754406	1862.599571	18.119488	-0.047370	2.428842
246.743365	1854.656253	18.124493	-0.047363	2.424226
246.604657	1846.713836	18.129498	-0.047332	2.419592
246.506011	1838.769923	18.134503	-0.047309	2.414951
246.525788	1830.801643	18.139507	-0.047307	2.410296
246.413766	1822.832113	18.144512	-0.047282	2.405621
246.554320	1814.885813	18.149517	-0.047303	2.400971
246.333468	1806.954302	18.154522	-0.047256	2.396291
246.223731	1798.983111	18.159527	-0.047231	2.391588
246.215925	1791.013807	18.164531	-0.047224	2.386885
246.123702	1783.046159	18.169536	-0.047202	2.382167
246.112431	1775.108792	18.174541	-0.047195	2.377463
245.725568	1767.189876	18.179546	-0.047118	2.372732
245.751939	1759.209036	18.184551	-0.047118	2.367987
245.870076	1751.252773	18.189555	-0.047134	2.363254
245.806352	1743.293995	18.194560	-0.047117	2.358496
245.707381	1735.345632	18.199565	-0.047094	2.353732
245.608821	1727.354848	18.204570	-0.047070	2.348932
245.604641	1719.382496	18.209575	-0.047065	2.344142
245.702446	1711.441646	18.214579	-0.047078	2.339369
245.545911	1703.495033	18.219584	-0.047043	2.334562
245.523060	1695.542877	18.224589	-0.047034	2.329752
245.279869	1687.601557	18.229594	-0.046984	2.324921
245.333118	1679.658400	18.234599	-0.046989	2.320104
245.365890	1671.705006	18.239603	-0.046990	2.315268
245.244619	1663.728333	18.244608	-0.046962	2.310395
245.317327	1655.757115	18.249613	-0.046970	2.305531
245.175251	1647.833826	18.254618	-0.046939	2.300669
244.999779	1639.900938	18.259623	-0.046901	2.295787
244.972627	1631.942614	18.264627	-0.046891	2.290892
244.849374	1623.993251	18.269632	-0.046863	2.285984
244.916514	1616.055797	18.274637	-0.046870	2.281089
244.724535	1608.116090	18.279642	-0.046829	2.276159
244.710479	1600.083913	18.284647	-0.046822	2.271177
244.899064	1592.089778	18.289651	-0.046852	2.266225
244.791546	1584.158201	18.294656	-0.046826	2.261276
244.666400	1576.255485	18.299661	-0.046798	2.256332
244.483083	1568.303710	18.304666	-0.046759	2.251341
244.474722	1560.343380	18.309671	-0.046752	2.246349
244.385271	1552.429637	18.314675	-0.046731	2.241369
244.376652	1544.475476	18.319680	-0.046724	2.236359
244.404283	1536.508877	18.324685	-0.046724	2.231332
244.131547	1528.580719	18.329690	-0.046668	2.226293
243.949760	1520.655752	18.334695	-0.046629	2.221252
244.058630	1512.704484	18.339699	-0.046644	2.216208
244.000991	1504.728983	18.344704	-0.046628	2.211123
243.910332	1496.800916	18.349709	-0.046606	2.206053
244.016149	1488.846424	18.354714	-0.046621	2.200973
243.956320	1480.912638	18.359719	-0.046605	2.195879
243.737152	1472.979023	18.364723	-0.046559	2.190758
243.656230	1465.001255	18.369728	-0.046539	2.185610
243.930494	1457.041563	18.374733	-0.046585	2.180494
243.644534	1449.141650	18.379738	-0.046526	2.175353
243.604409	1441.184406	18.384743	-0.046514	2.170185
243.507884	1433.255815	18.389747	-0.046491	2.165019
243.270542	1425.349975	18.394752	-0.046442	2.159842
243.448924	1417.389243	18.399757	-0.046470	2.154655
243.152084	1409.446545	18.404762	-0.046409	2.149423
243.274135	1401.471866	18.409767	-0.046427	2.144196
243.193316	1393.569690	18.414771	-0.046407	2.138986
242.974353	1385.637383	18.419776	-0.046361	2.133729
243.007496	1377.690262	18.424781	-0.046362	2.128474
242.911626	1369.753986	18.429786	-0.046339	2.123201
242.738052	1361.847947	18.434791	-0.046302	2.117927
243.037682	1353.834175	18.439795	-0.046352	2.112613
242.637049	1345.882496	18.444800	-0.046273	2.107260
242.655158	1337.964142	18.449805	-0.046271	2.101957
242.557461	1330.041168	18.454810	-0.046248	2.096625
242.497111	1322.106371	18.459815	-0.046231	2.091276
242.528038	1314.171280	18.464819	-0.046232	2.085922
242.294232	1306.273064	18.469824	-0.046183	2.080552
242.462219	1298.325511	18.474829	-0.046210	2.075175
242.312322	1290.376391	18.479834	-0.046177	2.069752
242.023028	1282.478110	18.484839	-0.046118	2.064335
242.257015	1274.528735	18.489843	-0.046156	2.058921
242.359998	1266.568289	18.494848	-0.046170	2.053472
242.002212	1258.687665	18.499853	-0.046099	2.048017
242.122648	1250.718214	18.504858	-0.046116	2.042534
241.980427	1242.836308	18.509863	-0.046084	2.037071
241.848443	1234.903739	18.514867	-0.046055	2.031559
241.795578	1226.933821	18.519872	-0.046040	2.026014
241.641547	1219.050289	18.524877	-0.046006	2.020503
241.536575	1211.132502	18.529882	-0.045981	2.014959
241.493096	1203.182999	18.534887	-0.045968	2.009383
241.446858	1195.273279	18.539891	-0.045954	2.003819
241.338042	1187.360959	18.544896	-0.045929	1.998232
241.328566	1179.427209	18.549901	-0.045922	1.992624
241.269967	1171.486114	18.554906	-0.045906	1.986990
241.246694	1163.564724	18.559911	-0.045897	1.981357
241.199307	1155.661565	18.564915	-0.045883	1.975719
241.169353	1147.710122	18.569920	-0.045872	1.970032
241.271175	1139.796545	18.574925	-0.045886	1.964370
241.207697	1131.887440	18.579930	-0.045869	1.958677
240.951151	1123.989374	18.584935	-0.045816	1.952955
240.983320	1116.028502	18.589939	-0.045817	1.947201
240.774536	1108.122082	18.594944	-0.045773	1.941444
240.667356	1100.228712	18.599949	-0.045748	1.935690
240.737913	1092.273400	18.604954	-0.045756	1.929893
240.704130	1084.360589	18.609959	-0.045745	1.924099
240.580488	1076.484944	18.614963	-0.045717	1.918304
240.310964	1068.574533	18.619968	-0.045662	1.912450
240.299665	1060.652679	18.624973	-0.045655	1.906598
240.176905	1052.749686	18.629978	-0.045627	1.900730
240.158047	1044.839279	18.634983	-0.045618	1.894849
240.216309	1036.908465	18.639987	-0.045624	1.888944
240.159303	1028.999033	18.644992	-0.045608	1.883023
240.098043	1021.122203	18.649997	-0.045592	1.877107
240.057824	1013.184378	18.655002	-0.045579	1.871130
239.921180	1005.265975	18.660007	-0.045549	1.865136
239.792087	997.398500	18.665011	-0.045520	1.859163
239.498948	989.513363	18.670016	-0.045460	1.853138
239.649884	981.572423	18.675021	-0.045483	1.847102
239.538743	973.687851	18.680026	-0.045457	1.841059
239.499875	965.790716	18.685031	-0.045445	1.834995
239.466290	957.881419	18.690035	-0.045434	1.828902
239.321366	949.978271	18.695040	-0.045402	1.822780
239.406820	942.085581	18.700045	-0.045412	1.816674
239.276853	934.183196	18.705050	-0.045383	1.810513
239.159345	926.299069	18.710055	-0.045356	1.804347
239.289829	918.407797	18.715059	-0.045375	1.798184
239.181748	910.479784	18.720064	-0.045350	1.791942
239.182191	902.556504	18.725069	-0.045345	1.785695
238.980963	894.699484	18.730074	-0.045303	1.779454
238.821479	886.824431	18.735079	-0.045268	1.773182
238.906018	878.908681	18.740083	-0.045279	1.766885
238.702713	871.053773	18.745088	-0.045236	1.760579
238.622639	863.192985	18.750093	-0.045216	1.754260
238.575678	855.280313	18.755098	-0.045202	1.747881
238.523482	847.396375	18.760103	-0.045187	1.741501
238.434400	839.534234	18.765107	-0.045166	1.735111
238.293666	831.646620	18.770112	-0.045134	1.728670
238.254042	823.778533	18.775117	-0.045122	1.722233
238.315233	815.894193	18.780122	-0.045128	1.715772
238.020648	808.025779	18.785127	-0.045068	1.709254
238.037285	800.138791	18.790131	-0.045066	1.702735
237.905978	792.274846	18.795136	-0.045037	1.696192
237.795614	784.408094	18.800141	-0.045011	1.689623
237.668425	776.542792	18.805146	-0.044983	1.683028
237.541716	768.690130	18.810151	-0.044954	1.676418
237.650084	760.785063	18.815155	-0.044969	1.669768
237.424293	752.932480	18.820160	-0.044922	1.663091
237.641538	745.043250	18.825165	-0.044957	1.656417
237.632382	737.175344	18.830170	-0.044951	1.649702
237.447830	729.336608	18.835175	-0.044911	1.642962
237.570449	721.469616	18.840179	-0.044929	1.636211
237.423850	713.565876	18.845184	-0.044897	1.629363
237.249761	705.731982	18.850189	-0.044859	1.622544
237.105197	697.898342	18.855194	-0.044827	1.615699
237.077396	690.027998	18.860199	-0.044817	1.608810
237.161403	682.167013	18.865203	-0.044828	1.601915
236.789466	674.377428	18.870208	-0.044753	1.594989
236.781631	666.506187	18.875213	-0.044747	1.588012
236.672304	658.672508	18.880218	-0.044722	1.581023
236.534263	650.846257	18.885223	-0.044691	1.574006
236.398803	643.008612	18.890227	-0.044661	1.566947
236.310539	635.174909	18.895232	-0.044639	1.559867
236.374649	627.325003	18.900237	-0.044646	1.552761
236.298341	619.458683	18.905242	-0.044627	1.545588
236.174721	611.651534	18.910247	-0.044599	1.538428
236.344729	603.785351	18.915251	-0.044625	1.531225
236.189200	595.970504	18.920256	-0.044591	1.523986
236.250678	588.146673	18.925261	-0.044598	1.516736
236.127423	580.317335	18.930266	-0.044570	1.509419
235.940581	572.519258	18.935271	-0.044530	1.502085
235.744400	564.739906	18.940275	-0.044489	1.494732
235.798014	556.887046	18.945280	-0.044494	1.487311
235.765393	549.091417	18.950285	-0.044483	1.479895
235.434675	541.306885	18.955290	-0.044416	1.472404
235.396292	533.450779	18.960295	-0.044404	1.464853
235.544666	525.635430	18.965299	-0.044426	1.457331
235.147139	517.874139	18.970304	-0.044347	1.449736
235.380813	510.036954	18.975309	-0.044386	1.442128
235.142857	502.276512	18.980314	-0.044337	1.434479
234.896309	494.493226	18.985319	-0.044286	1.426765
234.846070	486.716363	18.990323	-0.044271	1.419047
234.638122	478.937858	18.995328	-0.044228	1.411259
234.901203	471.104290	19.000333	-0.044272	1.403451
234.514658	463.386585	19.005338	-0.044195	1.395608
234.547674	455.565651	19.010343	-0.044196	1.387686
234.736181	447.766130	19.015347	-0.044226	1.379767
234.382461	440.033905	19.020352	-0.044155	1.371779
234.420709	432.259936	19.025357	-0.044157	1.363768
234.251891	424.521704	19.030362	-0.044121	1.355711
234.213766	416.749302	19.035367	-0.044109	1.347593
234.077283	409.016875	19.040371	-0.044078	1.339450
234.045668	401.248346	19.045376	-0.044068	1.331238
234.073939	393.502982	19.050381	-0.044068	1.323010
233.742013	385.794097	19.055386	-0.044001	1.314705
233.675448	377.928544	19.060391	-0.043984	1.306227
233.731995	370.203533	19.065395	-0.043989	1.297867
233.541523	362.491742	19.070400	-0.043949	1.289423
233.370225	354.803540	19.075405	-0.043912	1.280953
233.385642	347.085736	19.080410	-0.043910	1.272428
233.512389	339.333959	19.085415	-0.043929	1.263829
233.383201	331.665362	19.090419	-0.043900	1.255215
233.102258	323.986172	19.095424	-0.043842	1.246501
232.962417	316.330122	19.100429	-0.043812	1.237780
232.768166	308.635214	19.105434	-0.043770	1.228941
232.757230	300.931392	19.110439	-0.043763	1.220063
232.687736	293.259017	19.115443	-0.043746	1.211146
232.596672	285.588981	19.120448	-0.043724	1.202161
232.402350	277.959467	19.125453	-0.043683	1.193135
232.514263	270.254434	19.130458	-0.043699	1.184012
232.050992	262.676252	19.135463	-0.043607	1.174853
231.933405	255.031610	19.140467	-0.043581	1.165614
231.808406	247.409078	19.145472	-0.043552	1.156325
231.877118	239.711236	19.150477	-0.043560	1.146910
231.569703	232.125116	19.155482	-0.043498	1.137475
231.712409	224.462047	19.160487	-0.043520	1.127961
231.701160	216.862794	19.165491	-0.043513	1.118414
231.249913	209.314908	19.170496	-0.043424	1.108753
231.226095	201.721372	19.175501	-0.043415	1.099044
231.183643	194.129492	19.180506	-0.043402	1.089245
231.205709	186.547805	19.185511	-0.043401	1.079386
230.946057	179.020700	19.190515	-0.043348	1.069443
230.681408	171.483925	19.195520	-0.043294	1.059393
230.618735	163.943619	19.200525	-0.043278	1.049289
230.470532	156.423492	19.205530	-0.043245	1.039094
230.185361	148.934138	19.210535	-0.043187	1.028808
230.015814	141.441855	19.215539	-0.043151	1.018441
229.923326	133.931574	19.220544	-0.043129	1.007960
229.648780	126.490509	19.225549	-0.043073	0.997423
229.177480	119.035746	19.230554	-0.042980	0.986705
228.921438	111.592360	19.235559	-0.042928	0.975939
228.755133	104.146854	19.240563	-0.042892	0.965073
228.083113	96.801108	19.245568	-0.042762	0.954100
227.710433	89.411101	19.250573	-0.042688	0.943011
227.340438	82.039722	19.255578	-0.042615	0.931819
226.911831	74.692577	19.260583	-0.042530	0.920512
226.568118	67.349758	19.265587	-0.042461	0.909093
225.964219	60.286877	19.270592	-0.042344	0.897898