Tue Mar 23 11:46:37 2021

Number of Points = 3627
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.382373	0.096380	0.000000	0.000022	0.722602

0.653905	-0.034268	0.005005	-0.000029	0.722440
0.291405	-0.003231	0.010010	0.000039	0.722375
0.276413	0.003535	0.015014	0.000041	0.722383
0.318434	-0.005532	0.020019	0.000033	0.722380
0.288762	-0.001756	0.025024	0.000039	0.722377
0.429117	-0.024434	0.030029	0.000013	0.722382
0.356472	-0.017538	0.035034	0.000026	0.722370
0.513739	-0.041359	0.040038	-0.000003	0.722379
0.601222	-0.057366	0.045043	-0.000020	0.722378
0.410091	-0.024211	0.050048	0.000016	0.722376
0.530012	-0.042059	0.055053	-0.000006	0.722383
0.541495	-0.048113	0.060058	-0.000009	0.722376
0.413564	-0.022314	0.065062	0.000015	0.722382
0.431022	-0.026173	0.070067	0.000012	0.722380
0.566815	-0.052172	0.075072	-0.000014	0.722377
0.302906	-0.109125	0.080077	0.000035	0.722173
0.563498	-0.202745	0.085082	-0.000013	0.722080
0.523326	-0.192333	0.090086	-0.000006	0.722087
0.440439	-0.178606	0.095091	0.000010	0.722085
0.463885	-0.185437	0.100096	0.000005	0.722080
0.488706	-0.186675	0.105101	0.000001	0.722086
0.435981	-0.233288	0.110106	0.000010	0.721976
0.505078	-0.359194	0.115110	-0.000003	0.721753
0.662577	-0.387429	0.120115	-0.000032	0.721753
0.534269	-0.367243	0.125120	-0.000008	0.721748
0.619671	-0.376964	0.130125	-0.000024	0.721759
0.499507	-0.433220	0.135130	-0.000002	0.721606
0.639738	-0.538239	0.140134	-0.000028	0.721449
0.697390	-0.551119	0.145139	-0.000039	0.721444
0.579450	-0.531745	0.150144	-0.000017	0.721441
0.569934	-0.600285	0.155149	-0.000015	0.721303
0.647018	-0.704462	0.160154	-0.000029	0.721125
0.568399	-0.687248	0.165158	-0.000015	0.721132
0.372936	-0.654229	0.170163	0.000021	0.721128
0.366855	-0.753452	0.175168	0.000023	0.720931
0.455544	-0.790138	0.180173	0.000006	0.720890
0.251784	-0.757346	0.185178	0.000044	0.720883
0.370673	-0.840962	0.190182	0.000022	0.720761
0.452197	-0.962826	0.195187	0.000006	0.720549
0.308281	-0.940489	0.200192	0.000033	0.720543
0.184995	-0.947072	0.205197	0.000056	0.720487
0.309356	-1.103346	0.210202	0.000033	0.720223
0.333997	-1.103768	0.215206	0.000028	0.720231
0.301434	-1.139565	0.220211	0.000034	0.720149
0.253802	-1.257391	0.225216	0.000043	0.719900
0.320910	-1.263198	0.230221	0.000031	0.719913
0.377786	-1.354457	0.235226	0.000020	0.719753
0.142272	-1.384096	0.240230	0.000064	0.719612
0.249980	-1.404696	0.245235	0.000044	0.719609
0.041815	-1.517030	0.250240	0.000082	0.719315
0.039277	-1.533629	0.255245	0.000083	0.719281
-0.045185	-1.570415	0.260250	0.000098	0.719179
-0.169884	-1.655047	0.265254	0.000122	0.718969
-0.258620	-1.640271	0.270259	0.000138	0.718967
-0.214856	-1.772146	0.275264	0.000130	0.718722
-0.209445	-1.807698	0.280269	0.000129	0.718654
-0.228424	-1.859696	0.285274	0.000132	0.718545
-0.097275	-1.975447	0.290278	0.000108	0.718362
0.124833	-2.031196	0.295283	0.000066	0.718330
-0.116332	-2.146233	0.300288	0.000111	0.718019
-0.084853	-2.146621	0.305293	0.000105	0.718029
-0.155550	-2.285709	0.310298	0.000119	0.717729
-0.368497	-2.257496	0.315302	0.000158	0.717710
-0.442561	-2.368408	0.320307	0.000172	0.717465
-1.199504	-2.276305	0.325312	0.000313	0.717381
-2.353322	-2.125078	0.330317	0.000527	0.717274
-2.880135	-2.126841	0.335322	0.000625	0.717085
-2.632723	-2.168217	0.340326	0.000579	0.717090
-3.054350	-2.175476	0.345331	0.000658	0.716927
-4.154511	-2.066406	0.350336	0.000862	0.716756
-3.513757	-2.176258	0.355341	0.000743	0.716764
-3.913786	-2.142504	0.360346	0.000818	0.716690
-4.654610	-2.129160	0.365350	0.000955	0.716455
-4.285338	-2.195278	0.370355	0.000887	0.716455
-4.851338	-2.096561	0.375360	0.000992	0.716451
-4.731960	-2.222429	0.380365	0.000970	0.716244
-5.523125	-2.137771	0.385370	0.001117	0.716132
-5.671919	-2.108431	0.390374	0.001144	0.716138
-5.685041	-2.106525	0.395379	0.001147	0.716138
-5.753484	-2.173652	0.400384	0.001159	0.715980
-6.124306	-2.151904	0.405389	0.001228	0.715893
-6.432440	-2.101431	0.410394	0.001286	0.715884
-6.500458	-2.087030	0.415398	0.001298	0.715889
-6.382758	-2.163976	0.420403	0.001276	0.715778
-7.274244	-2.123828	0.425408	0.001442	0.715543
-7.186643	-2.133091	0.430413	0.001426	0.715556
-7.621128	-2.060465	0.435418	0.001507	0.715546
-7.154333	-2.141713	0.440422	0.001420	0.715550
-7.109397	-2.230185	0.445427	0.001411	0.715391
-8.683837	-2.030328	0.450432	0.001704	0.715231
-8.326364	-2.088960	0.455437	0.001638	0.715241
-8.427901	-2.075160	0.460442	0.001656	0.715233
-8.374652	-2.082950	0.465446	0.001646	0.715237
-7.869401	-2.190443	0.470451	0.001552	0.715202
-9.121621	-2.114758	0.475456	0.001785	0.714910
-9.342705	-2.072860	0.480461	0.001826	0.714915
-9.327395	-2.079319	0.485466	0.001824	0.714908
-8.857875	-2.160508	0.490470	0.001736	0.714913
-9.211681	-2.098390	0.495475	0.001802	0.714911
-9.403295	-2.087219	0.500480	0.001837	0.714865
-9.327482	-2.227921	0.505485	0.001823	0.714613
-9.826291	-2.142883	0.510490	0.001916	0.714606
-10.821221	-1.962519	0.515494	0.002101	0.714612
-10.261968	-2.062680	0.520499	0.001997	0.714611
-9.934089	-2.123555	0.525504	0.001936	0.714606
-9.952963	-2.121016	0.530509	0.001939	0.714605
-10.884299	-2.123246	0.535514	0.002113	0.714271
-11.063453	-2.087561	0.540518	0.002146	0.714279
-11.042969	-2.088496	0.545523	0.002142	0.714284
-10.942363	-2.110106	0.550528	0.002123	0.714277
-10.743019	-2.142233	0.555533	0.002086	0.714284
-11.026335	-2.096125	0.560538	0.002139	0.714275
-11.041684	-2.175319	0.565542	0.002142	0.714113
-11.878258	-2.096197	0.570547	0.002297	0.713974
-11.760301	-2.119208	0.575552	0.002275	0.713970
-11.936565	-2.083764	0.580557	0.002308	0.713978
-12.378263	-2.010579	0.585562	0.002390	0.713968
-11.667713	-2.135653	0.590566	0.002258	0.713971
-11.820054	-2.108043	0.595571	0.002286	0.713972
-12.867166	-2.053536	0.600576	0.002481	0.713709
-12.798107	-2.090914	0.605581	0.002468	0.713660
-12.612231	-2.128613	0.610586	0.002433	0.713651
-12.988350	-2.058747	0.615590	0.002503	0.713657
-12.971719	-2.061785	0.620595	0.002500	0.713657
-12.784558	-2.099125	0.625600	0.002465	0.713649
-12.570285	-2.130855	0.630605	0.002425	0.713662
-13.355108	-2.105784	0.635610	0.002571	0.713434
-13.674478	-2.084198	0.640614	0.002630	0.713364
-13.587616	-2.097550	0.645619	0.002614	0.713368
-13.874483	-2.051193	0.650624	0.002668	0.713359
-13.666578	-2.083361	0.655629	0.002629	0.713369
-13.759924	-2.070575	0.660634	0.002646	0.713361
-13.978100	-2.028687	0.665638	0.002687	0.713367
-14.186549	-2.088864	0.670643	0.002725	0.713174
-15.076288	-2.005025	0.675648	0.002891	0.713025
-14.560140	-2.092303	0.680653	0.002795	0.713035
-14.826447	-2.051644	0.685658	0.002844	0.713021
-14.745707	-2.061986	0.690662	0.002829	0.713030
-14.537827	-2.098152	0.695667	0.002790	0.713031
-14.827411	-2.050131	0.700672	0.002844	0.713024
-14.630771	-2.120679	0.705677	0.002808	0.712954
-15.397175	-2.105348	0.710682	0.002950	0.712713
-15.469341	-2.090530	0.715686	0.002964	0.712717
-15.803086	-2.031151	0.720691	0.003026	0.712717
-15.412677	-2.102539	0.725696	0.002953	0.712713
-15.133523	-2.147642	0.730701	0.002901	0.712723
-15.911053	-2.013791	0.735706	0.003045	0.712714
-15.613566	-2.108598	0.740710	0.002990	0.712630
-16.355753	-2.094112	0.745715	0.003128	0.712396
-16.446625	-2.080114	0.750720	0.003145	0.712392
-16.444947	-2.076571	0.755725	0.003145	0.712400
-16.665043	-2.042530	0.760730	0.003185	0.712389
-16.304407	-2.105991	0.765734	0.003118	0.712391
-16.549214	-2.062024	0.770739	0.003164	0.712392
-16.706956	-2.040696	0.775744	0.003193	0.712379
-16.888702	-2.147778	0.780749	0.003227	0.712101
-17.313679	-2.076372	0.785754	0.003306	0.712093
-17.175717	-2.098207	0.790758	0.003280	0.712098
-17.062303	-2.119114	0.795763	0.003259	0.712097
-17.791774	-1.993188	0.800768	0.003395	0.712089
-17.607067	-2.020766	0.805773	0.003360	0.712100
-17.316743	-2.077066	0.810778	0.003306	0.712091
-17.776998	-2.152826	0.815782	0.003392	0.711776
-18.348493	-2.056136	0.820787	0.003498	0.711766
-18.366002	-2.056301	0.825792	0.003501	0.711760
-17.808381	-2.150476	0.830797	0.003397	0.711770
-18.379647	-2.053670	0.835802	0.003503	0.711761
-18.649671	-2.003604	0.840806	0.003554	0.711765
-18.241335	-2.076075	0.845811	0.003478	0.711765
-18.754130	-2.112744	0.850816	0.003573	0.711510
-19.431057	-2.015105	0.855821	0.003699	0.711465
-19.414152	-2.022456	0.860826	0.003696	0.711456
-19.152080	-2.065506	0.865830	0.003647	0.711463
-19.177211	-2.060831	0.870835	0.003651	0.711464
-19.322790	-2.039782	0.875840	0.003678	0.711454
-19.003842	-2.091713	0.880845	0.003619	0.711464
-19.279646	-2.105393	0.885850	0.003670	0.711339
-20.103500	-2.056376	0.890854	0.003824	0.711144
-19.545918	-2.155206	0.895859	0.003720	0.711145
-20.315339	-2.021679	0.900864	0.003863	0.711138
-20.119350	-2.051355	0.905869	0.003826	0.711149
-19.910922	-2.094274	0.910874	0.003787	0.711138
-19.966413	-2.080436	0.915878	0.003798	0.711146
-20.054127	-2.138659	0.920883	0.003814	0.710998
-21.146176	-2.007296	0.925888	0.004017	0.710872
-20.570126	-2.105549	0.930893	0.003910	0.710881
-20.756224	-2.075165	0.935898	0.003944	0.710876
-21.017323	-2.025556	0.940902	0.003993	0.710882
-20.392514	-2.136405	0.945907	0.003877	0.710883
-20.648956	-2.095090	0.950912	0.003924	0.710875
-21.064857	-2.171159	0.955917	0.004002	0.710575
-21.729813	-2.071901	0.960922	0.004125	0.710537
-21.712884	-2.073118	0.965926	0.004122	0.710540
-21.573698	-2.096743	0.970931	0.004096	0.710543
-21.825141	-2.056902	0.975936	0.004143	0.710533
-21.678875	-2.077647	0.980941	0.004116	0.710544
-21.892585	-2.043552	0.985946	0.004155	0.710536
-22.639952	-2.065872	0.990950	0.004294	0.710225
-22.622058	-2.066754	0.995955	0.004291	0.710230
-23.014956	-2.001589	1.000960	0.004364	0.710221
-22.815752	-2.033019	1.005965	0.004327	0.710229
-22.854126	-2.028952	1.010970	0.004334	0.710224
-22.684474	-2.056405	1.015974	0.004302	0.710229
-22.783972	-2.038714	1.020979	0.004321	0.710229
-22.825852	-2.094188	1.025984	0.004328	0.710104
-23.402410	-2.089902	1.030989	0.004436	0.709907
-23.452259	-2.086052	1.035994	0.004445	0.709897
-23.888263	-2.003133	1.040998	0.004526	0.709908
-23.424772	-2.086262	1.046003	0.004440	0.709907
-23.246167	-2.123743	1.051008	0.004406	0.709896
-23.542881	-2.066228	1.056013	0.004461	0.709905
-23.620835	-2.123907	1.061018	0.004476	0.709762
-24.470446	-2.051137	1.066022	0.004634	0.709605
-24.124088	-2.112577	1.071027	0.004569	0.709606
-24.457252	-2.055552	1.076032	0.004631	0.709601
-24.298854	-2.081393	1.081037	0.004602	0.709606
-24.474428	-2.051667	1.086042	0.004634	0.709603
-24.783207	-1.996451	1.091046	0.004692	0.709604
-24.440541	-2.128812	1.096051	0.004628	0.709461
-25.462727	-2.042800	1.101056	0.004818	0.709269
-25.325411	-2.060832	1.106061	0.004793	0.709282
-25.433375	-2.044634	1.111066	0.004813	0.709276
-25.341725	-2.061820	1.116070	0.004795	0.709274
-25.509849	-2.030145	1.121075	0.004827	0.709278
-25.980626	-1.950662	1.126080	0.004914	0.709269
-25.376752	-2.054987	1.131085	0.004802	0.709276
-25.944176	-2.106109	1.136090	0.004907	0.708971
-26.793710	-1.958936	1.141094	0.005065	0.708963
-26.541253	-2.001776	1.146099	0.005018	0.708968
-26.002033	-2.101795	1.151104	0.004918	0.708960
-26.101010	-2.080258	1.156109	0.004936	0.708968
-26.346293	-2.042161	1.161114	0.004982	0.708957
-26.276214	-2.051957	1.166118	0.004969	0.708962
-26.194032	-2.172906	1.171123	0.004953	0.708750
-27.487529	-1.996836	1.176128	0.005194	0.708641
-26.870255	-2.102973	1.181133	0.005079	0.708649
-27.181684	-2.050631	1.186138	0.005137	0.708642
-27.645657	-1.967912	1.191142	0.005223	0.708643
-27.172119	-2.050188	1.196147	0.005135	0.708647
-27.206607	-2.047001	1.201152	0.005141	0.708641
-27.127281	-2.140635	1.206157	0.005126	0.708482
-28.041565	-2.041927	1.211162	0.005297	0.708354
-27.575638	-2.122889	1.216166	0.005210	0.708358
-27.897395	-2.066251	1.221171	0.005270	0.708357
-28.519019	-1.959409	1.226176	0.005385	0.708349
-28.142172	-2.020330	1.231181	0.005315	0.708361
-27.681592	-2.108127	1.236186	0.005229	0.708350
-28.602529	-2.081909	1.241190	0.005401	0.708074
-28.993430	-2.040699	1.246195	0.005473	0.708017
-28.873679	-2.063672	1.251200	0.005451	0.708014
-28.639926	-2.102251	1.256205	0.005407	0.708020
-29.256113	-1.995789	1.261210	0.005522	0.708014
-29.145616	-2.013338	1.266214	0.005501	0.708018
-28.494008	-2.129065	1.271219	0.005380	0.708019
-29.082324	-2.139525	1.276224	0.005489	0.707788
-29.863602	-2.039821	1.281229	0.005635	0.707709
-29.613722	-2.087617	1.286234	0.005588	0.707702
-30.045166	-2.008823	1.291238	0.005668	0.707706
-29.980302	-2.019096	1.296243	0.005656	0.707709
-30.016480	-2.017510	1.301248	0.005663	0.707699
-29.738761	-2.062564	1.306253	0.005611	0.707709
-29.836653	-2.127191	1.311258	0.005629	0.707544
-31.030181	-1.995884	1.316262	0.005851	0.707381
-30.353098	-2.113940	1.321267	0.005725	0.707386
-31.090443	-1.987473	1.326272	0.005862	0.707376
-30.988550	-1.999914	1.331277	0.005843	0.707388
-30.655374	-2.063060	1.336282	0.005781	0.707381
-30.817742	-2.033811	1.341286	0.005811	0.707381
-30.938522	-2.033125	1.346291	0.005834	0.707340
-31.472158	-2.065839	1.351296	0.005933	0.707083
-31.403205	-2.073073	1.356301	0.005920	0.707094
-32.032611	-1.965954	1.361306	0.006037	0.707084
-31.672195	-2.029212	1.366310	0.005970	0.707086
-31.310266	-2.093400	1.371315	0.005903	0.707086
-31.757797	-2.017295	1.376320	0.005986	0.707079
-31.673516	-2.034140	1.381325	0.005970	0.707076
-32.187521	-2.102235	1.386330	0.006066	0.706755
-32.634612	-2.019795	1.391334	0.006149	0.706761
-32.729452	-2.002308	1.396339	0.006167	0.706762
-32.502253	-2.048119	1.401344	0.006124	0.706752
-32.380227	-2.065047	1.406349	0.006101	0.706761
-32.493557	-2.047567	1.411354	0.006122	0.706756
-32.365166	-2.071613	1.416358	0.006098	0.706754
-33.024992	-2.099119	1.421363	0.006221	0.706463
-33.734978	-1.979648	1.426368	0.006353	0.706448
-33.405923	-2.034991	1.431373	0.006292	0.706455
-33.100789	-2.093409	1.436378	0.006235	0.706447
-33.305282	-2.056341	1.441382	0.006273	0.706449
-33.619091	-1.999635	1.446387	0.006331	0.706450
-33.649244	-1.997094	1.451392	0.006337	0.706445
-33.302327	-2.175273	1.456397	0.006272	0.706211
-34.416948	-2.015159	1.461402	0.006480	0.706134
-34.654553	-1.974013	1.466406	0.006524	0.706132
-34.118722	-2.068385	1.471411	0.006424	0.706134
-34.520250	-1.999343	1.476416	0.006499	0.706129
-34.470576	-2.001713	1.481421	0.006489	0.706142
-34.579941	-1.986605	1.486426	0.006510	0.706134
-34.431842	-2.079010	1.491430	0.006482	0.706001
-34.969307	-2.049099	1.496435	0.006582	0.705869
-34.813824	-2.078710	1.501440	0.006553	0.705865
-34.921883	-2.054949	1.506445	0.006573	0.705874
-35.141516	-2.019410	1.511450	0.006614	0.705867
-34.931599	-2.057559	1.516454	0.006575	0.705866
-34.723839	-2.113014	1.521459	0.006536	0.705829
-35.911776	-2.051926	1.526464	0.006757	0.705526
-35.891671	-2.052328	1.531469	0.006753	0.705532
-36.108986	-2.015804	1.536474	0.006794	0.705528
-35.805991	-2.069185	1.541478	0.006737	0.705529
-35.853428	-2.059410	1.546483	0.006746	0.705532
-36.441563	-1.958460	1.551488	0.006855	0.705525
-35.617263	-2.134846	1.556493	0.006702	0.705465
-36.515716	-2.100116	1.561498	0.006869	0.705213
-36.933493	-2.025302	1.566502	0.006947	0.705214
-36.919801	-2.024446	1.571507	0.006944	0.705221
-36.799175	-2.051099	1.576512	0.006921	0.705211
-36.621476	-2.077887	1.581517	0.006888	0.705221
-36.850716	-2.041057	1.586522	0.006931	0.705213
-36.837329	-2.104442	1.591526	0.006928	0.705090
-37.560588	-2.073863	1.596531	0.007063	0.704892
-37.517516	-2.084638	1.601536	0.007055	0.704886
-37.580705	-2.068996	1.606541	0.007067	0.704895
-37.910166	-2.014376	1.611546	0.007128	0.704887
-37.865808	-2.021971	1.616550	0.007119	0.704887
-37.478557	-2.089328	1.621555	0.007047	0.704891
-37.781034	-2.118965	1.626560	0.007104	0.704723
-38.802826	-1.999726	1.631565	0.007294	0.704596
-38.443855	-2.067310	1.636570	0.007227	0.704589
-38.358015	-2.081680	1.641574	0.007211	0.704591
-38.526875	-2.050070	1.646579	0.007242	0.704594
-38.695658	-2.023662	1.651584	0.007273	0.704587
-38.205325	-2.107226	1.656589	0.007182	0.704595
-38.674086	-2.133200	1.661594	0.007269	0.704374
-39.800996	-1.987408	1.666598	0.007479	0.704263
-39.450291	-2.046629	1.671603	0.007414	0.704270
-39.300172	-2.079231	1.676608	0.007386	0.704259
-39.314778	-2.073297	1.681613	0.007388	0.704265
-39.419939	-2.058731	1.686618	0.007408	0.704257
-39.151338	-2.104285	1.691622	0.007358	0.704262
-39.640082	-2.133798	1.696627	0.007449	0.704027
-40.619824	-1.995560	1.701632	0.007631	0.703954
-40.098543	-2.083333	1.706637	0.007534	0.703964
-40.104697	-2.088618	1.711642	0.007535	0.703951
-40.601003	-1.998098	1.716646	0.007627	0.703956
-40.094219	-2.086111	1.721651	0.007533	0.703961
-40.192503	-2.074432	1.726656	0.007551	0.703949
-40.748972	-2.110687	1.731661	0.007655	0.703676
-41.211539	-2.050000	1.736666	0.007741	0.703632
-41.344161	-2.024773	1.741670	0.007765	0.703635
-41.068564	-2.074440	1.746675	0.007714	0.703634
-41.530401	-1.994858	1.751680	0.007800	0.703629
-41.092385	-2.067600	1.756685	0.007718	0.703640
-41.018171	-2.084617	1.761690	0.007704	0.703632
-41.654484	-2.081178	1.766694	0.007823	0.703411
-42.337586	-1.992223	1.771699	0.007950	0.703344
-41.996248	-2.056663	1.776704	0.007886	0.703337
-41.778799	-2.090168	1.781709	0.007845	0.703348
-42.218963	-2.014408	1.786714	0.007927	0.703343
-42.167919	-2.024549	1.791718	0.007918	0.703341
-41.834348	-2.080764	1.796723	0.007856	0.703348
-42.549135	-2.070899	1.801728	0.007989	0.703110
-42.932982	-2.050533	1.806733	0.008060	0.703013
-42.819806	-2.074570	1.811738	0.008039	0.703006
-43.057524	-2.031998	1.816742	0.008083	0.703006
-42.936889	-2.050913	1.821747	0.008060	0.703012
-42.903517	-2.060724	1.826752	0.008054	0.703004
-42.928902	-2.051678	1.831757	0.008059	0.703013
-43.320143	-2.071777	1.836762	0.008132	0.702832
-43.960635	-2.026258	1.841766	0.008251	0.702693
-43.438540	-2.115314	1.846771	0.008154	0.702702
-43.976606	-2.025879	1.851776	0.008254	0.702689
-43.915607	-2.029415	1.856781	0.008242	0.702704
-43.679388	-2.073957	1.861786	0.008198	0.702699
-43.883954	-2.040307	1.866790	0.008236	0.702693
-44.238088	-2.059449	1.871795	0.008302	0.702527
-44.984731	-2.004930	1.876800	0.008441	0.702368
-44.537448	-2.079302	1.881805	0.008358	0.702379
-44.877454	-2.022817	1.886810	0.008421	0.702371
-45.032493	-1.996218	1.891814	0.008450	0.702369
-44.556589	-2.077160	1.896819	0.008361	0.702377
-45.151628	-1.974321	1.901824	0.008472	0.702371
-44.919301	-2.026543	1.906829	0.008428	0.702349
-45.407418	-2.075190	1.911834	0.008519	0.702075
-45.491058	-2.059583	1.916838	0.008535	0.702076
-45.599667	-2.039757	1.921843	0.008555	0.702078
-45.508674	-2.060182	1.926848	0.008538	0.702069
-45.427494	-2.070719	1.931853	0.008522	0.702077
-45.861136	-1.994643	1.936858	0.008603	0.702075
-45.461857	-2.116126	1.941862	0.008529	0.701973
-46.107831	-2.111684	1.946867	0.008649	0.701749
-46.681303	-2.013299	1.951872	0.008756	0.701742
-46.809815	-1.987109	1.956877	0.008779	0.701749
-46.525666	-2.040928	1.961882	0.008726	0.701742
-46.492636	-2.046584	1.966886	0.008720	0.701743
-46.867811	-1.976766	1.971891	0.008790	0.701749
-46.707987	-2.010579	1.976896	0.008760	0.701738
-46.634938	-2.168936	1.981901	0.008747	0.701444
-47.377983	-2.041317	1.986906	0.008885	0.701435
-47.622105	-1.996328	1.991910	0.008930	0.701438
-47.253448	-2.058237	1.996915	0.008861	0.701446
-47.579809	-2.002281	2.001920	0.008922	0.701441

-47.256657	-2.084435	2.011917	0.008862	0.701392
-48.333024	-2.023201	2.021914	0.009062	0.701127
-48.292650	-2.030975	2.031910	0.009054	0.701127
-48.304110	-2.029045	2.041907	0.009056	0.701127
-48.252507	-2.037123	2.051904	0.009047	0.701129
-48.268761	-2.035380	2.061901	0.009049	0.701127
-48.204982	-2.044704	2.071898	0.009037	0.701132
-47.491609	-2.071234	2.081894	0.008904	0.701336
-47.407909	-2.033018	2.091891	0.008889	0.701444
-47.355431	-2.043645	2.101888	0.008879	0.701442
-47.210697	-2.068983	2.111885	0.008852	0.701443
-47.539085	-2.010742	2.121882	0.008913	0.701443
-47.290768	-2.054663	2.131878	0.008866	0.701444
-47.292779	-2.054572	2.141875	0.008866	0.701443
-47.486097	-2.019293	2.151872	0.008902	0.701445
-46.844240	-2.032329	2.161869	0.008783	0.701651
-46.622859	-2.023112	2.171866	0.008741	0.701750
-46.389026	-2.065029	2.181862	0.008698	0.701750
-46.549293	-2.035951	2.191859	0.008727	0.701751
-46.174008	-2.104245	2.201856	0.008657	0.701748
-45.842656	-2.006952	2.211853	0.008595	0.702065
-45.348864	-2.089611	2.221850	0.008503	0.702076
-45.361274	-2.087126	2.231846	0.008505	0.702077
-45.547704	-2.053500	2.241843	0.008540	0.702078
-45.064921	-2.029536	2.251840	0.008450	0.702301
-44.849093	-2.033116	2.261837	0.008410	0.702372
-44.726050	-2.054507	2.271834	0.008386	0.702373
-44.654104	-2.053147	2.281830	0.008373	0.702402
-44.088680	-2.008176	2.291827	0.008267	0.702697
-43.824889	-2.055044	2.301824	0.008218	0.702698
-43.968369	-2.031203	2.311821	0.008245	0.702695
-43.584116	-2.026425	2.321818	0.008173	0.702843
-42.738344	-2.093963	2.331814	0.008015	0.703012
-43.239244	-2.004434	2.341811	0.008108	0.703013
-42.930198	-2.060297	2.351808	0.008051	0.703011
-42.359478	-2.014431	2.361805	0.007944	0.703310
-42.085638	-2.045170	2.371802	0.007893	0.703347
-42.079092	-2.045482	2.381798	0.007892	0.703349
-41.882335	-2.041308	2.391795	0.007855	0.703428
-41.206675	-2.055368	2.401792	0.007729	0.703643
-41.211001	-2.056026	2.411789	0.007730	0.703641
-41.331870	-2.033935	2.421786	0.007752	0.703642
-40.590052	-2.047087	2.431782	0.007614	0.703883
-40.624811	-2.001689	2.441779	0.007620	0.703962
-40.512789	-2.023126	2.451776	0.007599	0.703959
-40.327511	-1.998544	2.461773	0.007564	0.704076
-39.510989	-2.050704	2.471770	0.007412	0.704265
-39.603561	-2.033230	2.481766	0.007429	0.704267
-39.722092	-2.009153	2.491763	0.007451	0.704273
-38.967784	-1.981496	2.501760	0.007311	0.704600
-38.848524	-2.003991	2.511757	0.007288	0.704598
-38.667304	-2.039739	2.521754	0.007254	0.704591
-38.244407	-2.016308	2.531750	0.007175	0.704791
-37.927495	-2.022641	2.541747	0.007116	0.704892
-37.693405	-2.064866	2.551744	0.007073	0.704891
-38.079398	-1.971003	2.561741	0.007144	0.704942
-36.894299	-2.047517	2.571738	0.006923	0.705214
-36.913205	-2.044066	2.581734	0.006927	0.705214
-36.724142	-2.077838	2.591731	0.006891	0.705215
-36.614047	-2.004693	2.601728	0.006871	0.705402
-36.160926	-2.025043	2.611725	0.006786	0.705524
-36.076650	-2.038973	2.621722	0.006770	0.705526
-36.049690	-2.021332	2.631718	0.006765	0.705572
-35.247459	-2.017002	2.641715	0.006616	0.705868
-34.904461	-2.078091	2.651712	0.006552	0.705869
-35.463206	-1.980755	2.661709	0.006656	0.705864
-34.625056	-2.051851	2.671706	0.006499	0.706022
-34.473660	-2.023341	2.681702	0.006471	0.706134
-34.397496	-2.037494	2.691699	0.006457	0.706133
-34.476312	-1.993985	2.701696	0.006471	0.706193
-33.410523	-2.056936	2.711693	0.006273	0.706448
-33.485992	-2.044803	2.721690	0.006286	0.706446
-33.391112	-2.059726	2.731686	0.006269	0.706450
-32.900134	-2.045656	2.741683	0.006177	0.706655
-32.647210	-2.038220	2.751680	0.006130	0.706761
-32.741267	-2.025226	2.761677	0.006147	0.706753
-32.625954	-2.008819	2.771674	0.006125	0.706828
-31.815864	-2.023971	2.781670	0.005975	0.707088
-31.620007	-2.059766	2.791667	0.005938	0.707086
-32.023917	-1.988207	2.801664	0.006013	0.707086
-30.950368	-2.052906	2.811661	0.005813	0.707340
-31.024024	-2.020076	2.821658	0.005826	0.707380
-30.740553	-2.070589	2.831654	0.005774	0.707380
-30.643587	-2.044491	2.841651	0.005755	0.707468
-29.811949	-2.077102	2.851648	0.005600	0.707700
-30.013521	-2.039735	2.861645	0.005638	0.707703
-30.116804	-2.022688	2.871642	0.005657	0.707701
-29.283633	-2.056544	2.881638	0.005501	0.707931
-29.019395	-2.061660	2.891635	0.005452	0.708016
-29.096442	-2.048432	2.901632	0.005466	0.708015
-28.878231	-2.072349	2.911629	0.005425	0.708045
-28.307473	-2.021212	2.921626	0.005319	0.708352
-28.117671	-2.053587	2.931622	0.005284	0.708355
-27.935043	-2.086088	2.941619	0.005249	0.708356
-27.876620	-2.022718	2.951616	0.005238	0.708504
-27.450002	-2.031067	2.961613	0.005159	0.708640
-27.471469	-2.027510	2.971610	0.005163	0.708639
-27.297363	-2.031771	2.981606	0.005130	0.708693
-26.424502	-2.053204	2.991603	0.004967	0.708962
-26.423353	-2.054614	3.001600	0.004967	0.708960
-26.515982	-2.038494	3.011597	0.004984	0.708960
-25.931533	-2.036469	3.021594	0.004875	0.709173
-25.667086	-2.034904	3.031590	0.004826	0.709270
-25.582282	-2.049698	3.041587	0.004810	0.709271
-25.705253	-1.978077	3.051584	0.004832	0.709371
-24.710073	-2.040343	3.061581	0.004647	0.709602
-24.644379	-2.053489	3.071578	0.004635	0.709599
-24.827163	-2.018806	3.081574	0.004668	0.709604
-24.183009	-2.011646	3.091571	0.004548	0.709848
-24.107269	-2.000088	3.101568	0.004534	0.709898
-23.956064	-2.028627	3.111565	0.004506	0.709895
-23.729094	-1.986129	3.121562	0.004463	0.710061
-22.875542	-2.057481	3.131558	0.004304	0.710223
-23.046235	-2.026985	3.141555	0.004336	0.710224
-23.018839	-2.030688	3.151552	0.004331	0.710226
-22.244419	-2.013804	3.161549	0.004186	0.710536
-22.039985	-2.051044	3.171546	0.004148	0.710535
-21.896795	-2.075456	3.181542	0.004121	0.710537
-21.972528	-1.989900	3.191539	0.004135	0.710681
-21.031264	-2.059932	3.201536	0.003960	0.710877
-21.071624	-2.054654	3.211533	0.003967	0.710873
-21.198960	-2.031413	3.221530	0.003991	0.710875
-20.583153	-2.043939	3.231526	0.003876	0.711069
-20.522097	-2.017973	3.241523	0.003864	0.711143
-20.527006	-2.017211	3.251520	0.003865	0.711143
-20.302305	-1.991656	3.261517	0.003823	0.711274
-19.529626	-2.037906	3.271514	0.003679	0.711457
-19.470406	-2.049078	3.281510	0.003668	0.711456
-19.645701	-2.010243	3.291507	0.003700	0.711471
-18.565782	-2.055404	3.301504	0.003499	0.711765
-18.791206	-2.016375	3.311501	0.003541	0.711764
-18.638889	-2.043858	3.321498	0.003512	0.711763
-18.331924	-2.011732	3.331494	0.003455	0.711937
-17.674676	-2.048887	3.341491	0.003333	0.712096
-17.824783	-2.022414	3.351488	0.003360	0.712096
-17.946557	-1.990953	3.361485	0.003383	0.712116
-17.185104	-1.988958	3.371482	0.003241	0.712390
-16.790330	-2.058575	3.381478	0.003167	0.712392
-17.156426	-1.992762	3.391475	0.003235	0.712394
-16.119497	-2.059755	3.401472	0.003042	0.712628
-16.461055	-1.956839	3.411469	0.003105	0.712713
-15.932489	-2.050877	3.421466	0.003007	0.712713
-15.985299	-2.001985	3.431462	0.003017	0.712792
-15.084227	-2.041640	3.441459	0.002849	0.713033
-14.914151	-2.071735	3.451456	0.002817	0.713034
-15.114662	-2.037738	3.461453	0.002854	0.713031
-14.896106	-1.987850	3.471450	0.002813	0.713208
-14.091465	-2.050865	3.481446	0.002663	0.713368
-14.217655	-2.028184	3.491443	0.002686	0.713368
-13.965010	-2.074794	3.501440	0.002639	0.713366
-13.652573	-1.995927	3.511437	0.002581	0.713633
-13.247396	-2.056780	3.521434	0.002505	0.713656
-13.236066	-2.059028	3.531430	0.002503	0.713656
-13.181255	-2.003156	3.541427	0.002493	0.713787
-12.408970	-2.047950	3.551424	0.002349	0.713972
-12.764079	-1.985278	3.561421	0.002415	0.713971
-12.590743	-2.010487	3.571418	0.002382	0.713982
-11.759371	-2.008279	3.581414	0.002227	0.714281
-11.500336	-2.052959	3.591411	0.002179	0.714285
-11.621891	-2.032009	3.601408	0.002201	0.714283
-11.322890	-2.001200	3.611405	0.002146	0.714451
-10.610797	-2.048515	3.621402	0.002013	0.714609
-10.745334	-2.023640	3.631398	0.002038	0.714611
-10.649319	-2.039988	3.641395	0.002020	0.714613
-10.061234	-2.000009	3.651392	0.001910	0.714901
-9.806075	-2.039860	3.661389	0.001862	0.714912
-10.032016	-1.999689	3.671386	0.001904	0.714912
-9.529533	-2.002917	3.681382	0.001811	0.715084
-8.324633	-2.140133	3.691379	0.001586	0.715238
-8.462828	-2.115079	3.701376	0.001612	0.715239
-8.582254	-2.095417	3.711373	0.001634	0.715236
-8.374627	-2.087684	3.721370	0.001595	0.715325
-7.526301	-2.124793	3.731366	0.001437	0.715551
-7.542342	-2.120590	3.741363	0.001440	0.715554
-7.627137	-2.105126	3.751360	0.001455	0.715555
-7.547352	-2.070425	3.761357	0.001440	0.715653
-6.398584	-2.156569	3.771354	0.001226	0.715888
-6.526777	-2.132154	3.781350	0.001250	0.715891
-6.678704	-2.104852	3.791347	0.001278	0.715892
-6.651469	-2.067588	3.801344	0.001273	0.715976
-5.748457	-2.147451	3.811341	0.001105	0.716137
-5.785581	-2.141661	3.821338	0.001111	0.716135
-5.853468	-2.129840	3.831334	0.001124	0.716135
-5.299530	-2.121554	3.841331	0.001020	0.716347
-5.054826	-2.111115	3.851328	0.000975	0.716454
-4.983684	-2.124766	3.861325	0.000961	0.716453
-4.909061	-2.127632	3.871322	0.000947	0.716474
-4.286517	-2.094365	3.881318	0.000831	0.716759
-3.750315	-2.189418	3.891315	0.000731	0.716761
-4.003081	-2.143843	3.901312	0.000778	0.716762
-3.886658	-2.101996	3.911309	0.000756	0.716886
-3.230300	-2.117593	3.921306	0.000634	0.717087
-3.261406	-2.110704	3.931302	0.000640	0.717090
-3.204261	-2.121388	3.941299	0.000629	0.717089
-2.668078	-2.067193	3.951296	0.000529	0.717386
-2.312970	-2.131018	3.961293	0.000462	0.717385
-2.139031	-2.162738	3.971290	0.000430	0.717384
-2.335879	-2.054849	3.981286	0.000466	0.717528
-1.979686	-2.026854	3.991283	0.000400	0.717709
-1.706352	-2.075127	4.001280	0.000349	0.717710
-1.548176	-2.029993	4.011277	0.000319	0.717855
-1.131141	-2.019945	4.021274	0.000241	0.718022
-1.473203	-1.960647	4.031270	0.000305	0.718019
-1.071737	-1.933526	4.041267	0.000230	0.718215
-1.073590	-1.859960	4.051264	0.000230	0.718359
-1.525519	-1.749366	4.061261	0.000314	0.718419
-1.117108	-1.705970	4.071258	0.000238	0.718649
-0.933912	-1.718714	4.081254	0.000204	0.718688
-0.606069	-1.635780	4.091251	0.000142	0.718968
-0.535984	-1.641837	4.101248	0.000129	0.718981
-0.552066	-1.489284	4.111245	0.000132	0.719276
-0.565498	-1.458360	4.121242	0.000134	0.719333
-0.695461	-1.296911	4.131238	0.000158	0.719606
-0.314290	-1.284820	4.141235	0.000087	0.719764
-0.234928	-1.226982	4.151232	0.000072	0.719906
-0.429234	-1.044049	4.161229	0.000108	0.720199
-0.331668	-0.973419	4.171226	0.000089	0.720372
-0.325279	-0.877008	4.181222	0.000088	0.720565
-0.118255	-0.752689	4.191219	0.000049	0.720882
-0.195911	-0.651055	4.201216	0.000064	0.721055
-0.147066	-0.556310	4.211213	0.000054	0.721259
-0.139162	-0.430999	4.221210	0.000052	0.721509
-0.188213	-0.289342	4.231206	0.000061	0.721770
-0.048262	-0.154797	4.241203	0.000035	0.722084
-0.026489	-0.019158	4.251200	0.000031	0.722358
-0.049001	0.133414	4.261197	0.000035	0.722650
0.000000	0.290321	4.271194	0.000025	0.722976

0.123481	0.907376	4.276198	0.000002	0.724229
0.310722	2.135572	4.281203	-0.000034	0.726696
0.370409	3.976008	4.286208	-0.000046	0.730302
0.790998	6.313993	4.291213	-0.000126	0.734975
1.011627	9.189631	4.296218	-0.000169	0.740580
1.248610	12.550681	4.301222	-0.000216	0.747072
1.640884	16.331724	4.306227	-0.000291	0.754350
2.095642	20.506577	4.311232	-0.000379	0.762312
2.407321	25.113506	4.316237	-0.000440	0.770940
2.685685	30.087658	4.321242	-0.000495	0.780130
3.304440	35.354578	4.326246	-0.000614	0.789847
3.672210	40.985303	4.331251	-0.000686	0.800013
3.932433	46.929173	4.336256	-0.000738	0.810566
4.717864	53.070407	4.341261	-0.000889	0.821484
5.292840	59.524176	4.346266	-0.001000	0.832728
5.544357	66.250762	4.351270	-0.001051	0.844184
6.038464	73.166335	4.356275	-0.001148	0.855871
6.525972	80.271900	4.361280	-0.001243	0.867709
7.312465	87.531148	4.366285	-0.001395	0.879721
8.024132	94.970008	4.371290	-0.001532	0.891834
8.687598	102.582673	4.376294	-0.001661	0.904045
9.152183	110.381196	4.381299	-0.001752	0.916326
9.671532	118.271944	4.386304	-0.001854	0.928599
10.445131	126.254509	4.391309	-0.002004	0.940918
11.631840	134.264702	4.396314	-0.002230	0.953226
15.565334	141.958630	4.401318	-0.002967	0.965616
16.141389	150.327175	4.406323	-0.003080	0.977976
16.950023	158.719269	4.411328	-0.003236	0.990273
17.647768	167.174612	4.416333	-0.003372	1.002481
18.429484	175.649733	4.421338	-0.003523	1.014590
19.164452	184.172730	4.426342	-0.003665	1.026610
20.113242	192.708473	4.431347	-0.003848	1.038559
20.904171	201.286423	4.436352	-0.004001	1.050391
22.488065	209.767530	4.441357	-0.004301	1.062145
23.514478	218.380921	4.446362	-0.004498	1.073817
24.182314	227.047627	4.451366	-0.004628	1.085351
25.175048	235.680973	4.456371	-0.004819	1.096793
25.966179	244.339588	4.461376	-0.004972	1.108105
27.092406	252.957972	4.466381	-0.005187	1.119323
27.999397	261.614174	4.471386	-0.005362	1.130430
28.721117	270.299610	4.476390	-0.005502	1.141426
29.520884	278.987120	4.481395	-0.005656	1.152334
30.523356	287.585069	4.486400	-0.005849	1.163074
31.819815	296.147745	4.491405	-0.006096	1.173732
33.022368	304.708020	4.496410	-0.006325	1.184272
33.773953	313.359898	4.501414	-0.006471	1.194736
34.844086	321.919324	4.506419	-0.006676	1.205063
35.718715	330.519809	4.511424	-0.006845	1.215312
36.319151	339.146816	4.516429	-0.006962	1.225451
36.890206	347.781110	4.521434	-0.007074	1.235509
37.711542	356.311842	4.526438	-0.007233	1.245416
38.726591	364.822554	4.531443	-0.007427	1.255259
39.507560	373.349266	4.536448	-0.007578	1.264998
40.196168	381.907362	4.541453	-0.007712	1.274680
40.699481	390.441525	4.546458	-0.007812	1.284228
41.360771	398.958312	4.551462	-0.007940	1.293716
42.287926	407.399158	4.556467	-0.008119	1.303100
42.819990	415.977844	4.561472	-0.008223	1.312493
43.823217	424.411397	4.566477	-0.008416	1.321749
44.481742	432.829735	4.571482	-0.008544	1.330862
45.296427	441.233046	4.576486	-0.008701	1.339925
45.735509	449.685734	4.581491	-0.008788	1.348913
46.254587	458.110335	4.586496	-0.008891	1.357825
47.076726	466.466840	4.591501	-0.009049	1.366661
47.569132	474.886345	4.596506	-0.009147	1.375448
48.200786	483.257223	4.601510	-0.009270	1.384153
48.947000	491.629244	4.606515	-0.009414	1.392823
49.695527	499.944183	4.611520	-0.009559	1.401383
50.049537	508.345047	4.616525	-0.009630	1.409911
50.267748	516.748737	4.621530	-0.009677	1.418368
50.878118	525.055127	4.626534	-0.009796	1.426742
51.748370	533.356732	4.631539	-0.009963	1.435105
52.247294	541.673152	4.636544	-0.010062	1.443373
53.026027	549.974116	4.641549	-0.010212	1.451624
53.768694	558.261190	4.646554	-0.010356	1.459809
54.359492	566.575972	4.651558	-0.010471	1.467951
54.806534	574.955487	4.656563	-0.010560	1.476086
55.338674	583.211997	4.661568	-0.010665	1.484074
56.028776	591.489263	4.666573	-0.010799	1.492062
56.450237	599.769602	4.671578	-0.010883	1.499969
57.146942	608.012005	4.676582	-0.011018	1.507841
57.846697	616.277236	4.681587	-0.011154	1.515693
58.371124	624.527505	4.686592	-0.011257	1.523464
58.944361	632.800385	4.691597	-0.011369	1.531224
59.401317	641.073150	4.696602	-0.011460	1.538927
60.214604	649.278298	4.701606	-0.011616	1.546583
60.895222	657.551761	4.706611	-0.011749	1.554243
61.325518	665.790866	4.711616	-0.011834	1.561797
62.110094	673.994592	4.716621	-0.011986	1.569335
62.539278	682.261112	4.721626	-0.012071	1.576841
62.957735	690.503325	4.726630	-0.012154	1.584288
63.594302	698.731388	4.731635	-0.012278	1.591719
63.778230	706.996487	4.736640	-0.012318	1.599084
64.349094	715.207104	4.741645	-0.012430	1.606421
64.869731	723.426847	4.746650	-0.012532	1.613726
65.566835	731.616059	4.751654	-0.012667	1.620995
66.099064	739.837813	4.756659	-0.012772	1.628238
66.403367	748.130670	4.761664	-0.012834	1.635478
67.156259	756.275309	4.766669	-0.012980	1.642620
67.413307	764.502647	4.771674	-0.013033	1.649734
67.779183	772.711281	4.776678	-0.013107	1.656816
68.452526	780.868531	4.781683	-0.013237	1.663865
68.876287	789.052843	4.786688	-0.013322	1.670874
69.680237	797.198134	4.791693	-0.013477	1.677872
70.049611	805.380582	4.796698	-0.013551	1.684813
70.529597	813.578996	4.801702	-0.013646	1.691754
70.790315	821.807653	4.806707	-0.013700	1.698663
71.100372	829.983401	4.811712	-0.013763	1.705507
71.446932	838.201708	4.816717	-0.013833	1.712362
71.960878	846.344050	4.821722	-0.013934	1.719150
72.244237	854.527935	4.826726	-0.013992	1.725915
72.602614	862.719705	4.831731	-0.014064	1.732669
73.187474	870.844544	4.836736	-0.014178	1.739372
73.525733	879.020467	4.841741	-0.014247	1.746058
73.689919	887.226119	4.846746	-0.014283	1.752721
74.235398	895.355834	4.851750	-0.014390	1.759346
75.043373	903.447853	4.856755	-0.014546	1.765948
75.241001	911.651468	4.861760	-0.014588	1.772539
76.029847	919.769095	4.866765	-0.014740	1.779109
76.682272	927.881028	4.871770	-0.014867	1.785634
77.046139	936.107725	4.876774	-0.014940	1.792191
77.386571	944.301145	4.881779	-0.015009	1.798694
77.707904	952.412307	4.886784	-0.015074	1.805107
78.209680	960.565943	4.891789	-0.015173	1.811552
78.694552	968.698621	4.896794	-0.015269	1.817956
79.252791	976.817192	4.901798	-0.015378	1.824335
79.593555	984.992319	4.906803	-0.015447	1.830709
80.034313	993.129696	4.911808	-0.015534	1.837044
80.591569	1001.242579	4.916813	-0.015643	1.843352
80.889469	1009.403738	4.921818	-0.015704	1.849644
81.075331	1017.580053	4.926822	-0.015744	1.855914
81.580570	1025.687390	4.931827	-0.015844	1.862147
82.164580	1033.794916	4.936832	-0.015958	1.868369
82.496346	1041.986852	4.941837	-0.016025	1.874604
82.898310	1050.090574	4.946842	-0.016105	1.880761
83.328847	1058.204621	4.951846	-0.016191	1.886908
83.939422	1066.321770	4.956851	-0.016310	1.893057
84.405475	1074.438369	4.961856	-0.016402	1.899170
85.027165	1082.530693	4.966861	-0.016523	1.905263
85.394546	1090.694893	4.971866	-0.016597	1.911361
86.256953	1098.766601	4.976870	-0.016763	1.917426
86.692015	1106.890472	4.981875	-0.016849	1.923462
86.902435	1115.052814	4.986880	-0.016894	1.929483
87.357172	1123.195164	4.991885	-0.016984	1.935498
87.670110	1131.311333	4.996890	-0.017047	1.941459
87.895277	1139.459460	5.001894	-0.017095	1.947416
88.412359	1147.614887	5.006899	-0.017196	1.953391
88.785406	1155.713366	5.011904	-0.017271	1.959291
89.318206	1163.779361	5.016909	-0.017376	1.965167
89.774939	1171.884798	5.021914	-0.017466	1.971046
90.052524	1180.032371	5.026918	-0.017523	1.976918
90.703509	1188.093556	5.031923	-0.017650	1.982750
91.309575	1196.175630	5.036928	-0.017768	1.988575
91.631336	1204.355567	5.041933	-0.017833	1.994423
91.970644	1212.441388	5.046938	-0.017902	2.000189
92.432636	1220.531804	5.051942	-0.017993	2.005954
92.648676	1228.675363	5.056947	-0.018039	2.011714
93.026592	1236.786089	5.061952	-0.018115	2.017452
93.561342	1244.873247	5.066957	-0.018219	2.023172
94.119082	1252.949040	5.071962	-0.018329	2.028871
94.318744	1261.121511	5.076966	-0.018371	2.034585
94.668965	1269.207052	5.081971	-0.018442	2.040237
95.071542	1277.272667	5.086976	-0.018522	2.045865
95.292292	1285.410077	5.091981	-0.018569	2.051509
95.778538	1293.494754	5.096986	-0.018665	2.057128
96.100613	1301.582906	5.101990	-0.018730	2.062717
96.466445	1309.690085	5.106995	-0.018803	2.068308
96.796006	1317.804433	5.112000	-0.018870	2.073886
97.553465	1325.838098	5.117005	-0.019016	2.079436
97.798827	1333.949788	5.122010	-0.019067	2.084973
98.194775	1342.058424	5.127014	-0.019147	2.090508
98.717311	1350.156680	5.132019	-0.019249	2.096034
99.083832	1358.236931	5.137024	-0.019323	2.101518
99.323870	1366.365453	5.142029	-0.019373	2.107008
99.551200	1374.526067	5.147034	-0.019421	2.112503
99.979084	1382.606821	5.152038	-0.019506	2.117951
100.492798	1390.654220	5.157043	-0.019607	2.123370
100.537959	1398.752765	5.162048	-0.019620	2.128764
101.140210	1406.822861	5.167053	-0.019738	2.134179
101.504906	1414.902628	5.172058	-0.019811	2.139564
101.763953	1422.987392	5.177062	-0.019865	2.144929
101.916640	1431.117522	5.182067	-0.019898	2.150300
102.532418	1439.158792	5.187072	-0.020018	2.155643
103.130802	1447.214624	5.192077	-0.020135	2.160980
103.379737	1455.312330	5.197082	-0.020187	2.166299
103.643144	1463.414427	5.202086	-0.020241	2.171609
104.252673	1471.504777	5.207091	-0.020360	2.176930
104.359185	1479.597545	5.212096	-0.020385	2.182193
104.759569	1487.684798	5.217101	-0.020465	2.187467
105.197733	1495.790660	5.222106	-0.020552	2.192744
105.468943	1503.879060	5.227110	-0.020608	2.197981
105.969603	1511.924757	5.232115	-0.020707	2.203200
106.234253	1519.997514	5.237120	-0.020761	2.208402
106.704637	1528.087244	5.242125	-0.020854	2.213620
106.837090	1536.182607	5.247130	-0.020884	2.218800
107.091043	1544.259373	5.252134	-0.020937	2.223967
107.714526	1552.303694	5.257139	-0.021058	2.229134
107.783987	1560.431930	5.262144	-0.021076	2.234293
108.308896	1568.480919	5.267149	-0.021180	2.239430
108.814616	1576.531145	5.272154	-0.021279	2.244554
109.443406	1584.573102	5.277158	-0.021401	2.249672
109.812305	1592.689076	5.282163	-0.021476	2.254803
110.145020	1600.768482	5.287168	-0.021543	2.259895
110.773087	1608.816724	5.292173	-0.021665	2.264982
111.176900	1616.912767	5.297178	-0.021746	2.270067
111.555332	1625.072445	5.302182	-0.021821	2.275179
111.848016	1633.124184	5.307187	-0.021881	2.280205
111.974156	1641.196655	5.312192	-0.021910	2.285218
112.117564	1649.279274	5.317197	-0.021942	2.290228
112.638593	1657.325089	5.322202	-0.022045	2.295237
112.918739	1665.383031	5.327206	-0.022102	2.300221
113.244768	1673.449071	5.332211	-0.022168	2.305203
113.457737	1681.534486	5.337216	-0.022213	2.310177
113.972508	1689.601666	5.342221	-0.022314	2.315155
114.258835	1697.663680	5.347226	-0.022373	2.320099
114.616389	1705.720066	5.352230	-0.022445	2.325035
115.142516	1713.787641	5.357235	-0.022548	2.329981
115.297926	1721.884635	5.362240	-0.022582	2.334905
115.618072	1729.958701	5.367245	-0.022647	2.339817
115.987745	1738.014283	5.372250	-0.022722	2.344712
116.304815	1746.087844	5.377254	-0.022786	2.349603
116.586058	1754.225124	5.382259	-0.022844	2.354519
116.709153	1762.261865	5.387264	-0.022872	2.359352
117.293439	1770.296207	5.392269	-0.022986	2.364210
117.770215	1778.335773	5.397274	-0.023080	2.369053
117.917505	1786.447044	5.402278	-0.023113	2.373903
118.150483	1794.523108	5.407283	-0.023162	2.378728
118.600833	1802.534063	5.412288	-0.023251	2.383522
118.773680	1810.630399	5.417293	-0.023288	2.388335
119.043672	1818.707529	5.422298	-0.023344	2.393135
119.646145	1826.732726	5.427302	-0.023461	2.397920
120.038235	1834.779784	5.432307	-0.023540	2.402693
120.178165	1842.841763	5.437312	-0.023571	2.407444
120.712376	1850.912791	5.442317	-0.023676	2.412222
121.032657	1858.989541	5.447322	-0.023741	2.416978
121.087598	1867.078447	5.452326	-0.023756	2.421711
121.617219	1875.117125	5.457331	-0.023860	2.426441
122.017365	1883.201514	5.462336	-0.023940	2.431179
122.247586	1891.335051	5.467341	-0.023989	2.435923
122.519365	1899.361958	5.472346	-0.024044	2.440600
122.891958	1907.369363	5.477350	-0.024119	2.445263
123.167518	1915.449903	5.482355	-0.024176	2.449953
123.315256	1923.530581	5.487360	-0.024209	2.454624
123.710751	1931.566727	5.492365	-0.024288	2.459279
124.167013	1939.576445	5.497370	-0.024378	2.463914
124.489318	1947.651138	5.502374	-0.024443	2.468568
124.849478	1955.741555	5.507379	-0.024516	2.473225
125.199733	1963.776261	5.512384	-0.024586	2.477841
125.405743	1971.839936	5.517389	-0.024630	2.482454
125.612951	1979.887021	5.522394	-0.024674	2.487048
125.873339	1987.972244	5.527398	-0.024728	2.491660
126.107968	1996.062992	5.532403	-0.024777	2.496265
126.501819	2004.067169	5.537408	-0.024855	2.500823
127.194378	2012.091507	5.542413	-0.024989	2.505407
127.706633	2020.140276	5.547418	-0.025090	2.509982
128.003354	2028.260560	5.552422	-0.025151	2.514574
128.269345	2036.328062	5.557427	-0.025206	2.519125
128.535072	2044.343776	5.562432	-0.025260	2.523639
128.899200	2052.426777	5.567437	-0.025334	2.528190
128.985031	2060.499909	5.572442	-0.025355	2.532707
129.243747	2068.554045	5.577446	-0.025408	2.537218
129.686175	2076.601602	5.582451	-0.025496	2.541730
129.798502	2084.645996	5.587456	-0.025522	2.546208
130.076912	2092.728106	5.592461	-0.025580	2.550712
130.309568	2100.802534	5.597466	-0.025628	2.555200
130.747982	2108.795544	5.602470	-0.025715	2.559649
131.096806	2116.846018	5.607475	-0.025785	2.564117
131.203215	2124.919696	5.612480	-0.025811	2.568572
131.629629	2132.976650	5.617485	-0.025895	2.573032
131.917987	2141.031018	5.622490	-0.025954	2.577474
132.185247	2149.069038	5.627494	-0.026009	2.581897
132.444687	2157.136843	5.632499	-0.026063	2.586329
132.585553	2165.227444	5.637504	-0.026095	2.590757
132.972973	2173.441100	5.642509	-0.026172	2.595262
133.182757	2181.414372	5.647514	-0.026217	2.599616
133.395000	2189.415216	5.652518	-0.026261	2.603978
133.867271	2197.435669	5.657523	-0.026355	2.608360
134.168000	2205.466047	5.662528	-0.026416	2.612729
134.559987	2213.508888	5.667533	-0.026494	2.617104
134.656613	2221.570625	5.672538	-0.026518	2.621461
134.921881	2229.586207	5.677542	-0.026572	2.625798
135.382898	2237.629751	5.682547	-0.026663	2.630155
135.819551	2245.680603	5.687552	-0.026750	2.634508
136.121500	2253.725426	5.692557	-0.026812	2.638841
136.568622	2261.745454	5.697562	-0.026900	2.643163
136.641724	2269.810281	5.702566	-0.026919	2.647477
136.964176	2277.880725	5.707571	-0.026984	2.651804
137.216948	2285.929924	5.712576	-0.027037	2.656107
137.476155	2294.000954	5.717581	-0.027090	2.660416
137.688666	2302.026164	5.722586	-0.027135	2.664690
137.957301	2310.071736	5.727590	-0.027191	2.668972
138.324107	2318.179325	5.732595	-0.027264	2.673286
138.462910	2326.200646	5.737600	-0.027295	2.677533
138.731812	2334.241009	5.742605	-0.027351	2.681792
139.159855	2342.259128	5.747610	-0.027436	2.686041
139.306000	2350.312226	5.752614	-0.027468	2.690285
139.745916	2358.373807	5.757619	-0.027556	2.694545
139.891514	2366.422296	5.762624	-0.027588	2.698773
140.224367	2374.455118	5.767629	-0.027655	2.702998
140.473422	2382.503547	5.772634	-0.027707	2.707219
140.790266	2390.555406	5.777638	-0.027771	2.711439
141.059109	2398.650312	5.782643	-0.027827	2.715672
141.183302	2406.665270	5.787648	-0.027855	2.719848
141.489044	2414.689127	5.792653	-0.027917	2.724033
141.825539	2422.740546	5.797658	-0.027985	2.728228
142.028453	2430.798032	5.802662	-0.028029	2.732412
142.267451	2438.867962	5.807667	-0.028078	2.736598
142.354920	2446.911350	5.812672	-0.028100	2.740754
142.862858	2454.917512	5.817677	-0.028200	2.744910
143.002363	2462.977583	5.822682	-0.028231	2.749066
143.350180	2471.087534	5.827686	-0.028301	2.753253
143.788237	2479.126377	5.832691	-0.028388	2.757403
143.725170	2487.169688	5.837696	-0.028382	2.761518
143.988813	2495.174617	5.842701	-0.028436	2.765628
144.311283	2503.179859	5.847706	-0.028502	2.769735
144.461613	2511.253353	5.852710	-0.028535	2.773860
144.904750	2519.274269	5.857715	-0.028623	2.777970
144.932555	2527.320446	5.862720	-0.028633	2.782062
145.481781	2535.337837	5.867725	-0.028741	2.786164
145.732871	2543.388866	5.872730	-0.028793	2.790260
145.611223	2551.496104	5.877734	-0.028776	2.794356
146.043115	2559.507542	5.882739	-0.028861	2.798430
146.146715	2567.526543	5.887744	-0.028886	2.802482
146.175102	2575.601191	5.892749	-0.028896	2.806553
146.112133	2583.680045	5.897754	-0.028890	2.810614
146.518073	2591.692058	5.902758	-0.028971	2.814663
146.711397	2599.750079	5.907763	-0.029012	2.818717
146.896741	2607.749012	5.912768	-0.029052	2.822735
147.224840	2615.800040	5.917773	-0.029119	2.826781
147.529346	2623.851716	5.922778	-0.029181	2.830821
147.906677	2631.908692	5.927782	-0.029256	2.834861
148.408796	2639.908064	5.932787	-0.029355	2.838874
148.811654	2647.913926	5.937792	-0.029435	2.842879
148.888238	2655.986979	5.942797	-0.029455	2.846894
149.211563	2664.021020	5.947802	-0.029520	2.850897
149.651776	2672.046463	5.952806	-0.029608	2.854896
149.586345	2680.140144	5.957811	-0.029601	2.858896
149.705472	2688.150455	5.962816	-0.029628	2.862859
149.954167	2696.211925	5.967821	-0.029680	2.866849
150.247057	2704.262712	5.972826	-0.029740	2.870830
150.327624	2712.312930	5.977830	-0.029760	2.874794
150.848611	2720.318332	5.982835	-0.029862	2.878755
150.927370	2728.335104	5.987840	-0.029882	2.882691
151.167961	2736.399164	5.992845	-0.029933	2.886655
151.262132	2744.454877	5.997850	-0.029955	2.890600
151.531158	2752.497230	6.002854	-0.030011	2.894543
151.854965	2760.551069	6.007859	-0.030076	2.898489
152.138623	2768.544812	6.012864	-0.030135	2.902399
152.407562	2776.604411	6.017869	-0.030190	2.906334
152.527340	2784.653503	6.022874	-0.030218	2.910251
152.702815	2792.788550	6.027878	-0.030256	2.914207
153.165828	2800.778251	6.032883	-0.030347	2.918103
153.427272	2808.775041	6.037888	-0.030401	2.921986
153.596085	2816.803691	6.042893	-0.030438	2.925874
153.770966	2824.831455	6.047898	-0.030476	2.929758
154.213553	2832.867513	6.052902	-0.030563	2.933653
154.329391	2840.930403	6.057907	-0.030590	2.937540
154.214158	2848.993914	6.062912	-0.030574	2.941410
154.750225	2856.957380	6.067917	-0.030679	2.945260
155.067576	2865.006596	6.072922	-0.030744	2.949135
155.389763	2873.047784	6.077926	-0.030809	2.953001
155.654292	2881.091503	6.082931	-0.030864	2.956861
155.934859	2889.122571	6.087936	-0.030921	2.960710
155.853420	2897.171496	6.092941	-0.030911	2.964544
155.988660	2905.218839	6.097946	-0.030942	2.968384
156.222503	2913.238594	6.102950	-0.030991	2.972210
156.660074	2921.296484	6.107955	-0.031077	2.976060
156.677881	2929.295004	6.112960	-0.031086	2.979855
157.178168	2937.323851	6.117965	-0.031185	2.983684
157.419748	2945.374788	6.122970	-0.031235	2.987506
157.607192	2953.447170	6.127974	-0.031275	2.991330
157.883139	2961.521992	6.132979	-0.031332	2.995155
157.840589	2969.519484	6.137984	-0.031329	2.998922
158.112191	2977.551790	6.142989	-0.031385	3.002717
158.257937	2985.573037	6.147994	-0.031418	3.006496
158.581381	2993.569252	6.152998	-0.031483	3.010266
158.825766	3001.675843	6.158003	-0.031534	3.014080
158.820942	3009.688066	6.163008	-0.031538	3.017833
159.170158	3017.738911	6.168013	-0.031609	3.021616
159.451421	3025.739555	6.173018	-0.031666	3.025368
159.647805	3033.769115	6.178022	-0.031708	3.029124
160.017766	3041.839745	6.183027	-0.031782	3.032904
160.295762	3049.856975	6.188032	-0.031839	3.036649
160.565525	3057.879727	6.193037	-0.031895	3.040391
160.772609	3065.894732	6.198042	-0.031939	3.044123
161.010268	3073.920593	6.203046	-0.031988	3.047856
161.577554	3081.976639	6.208051	-0.032099	3.051614
161.496325	3090.044349	6.213056	-0.032090	3.055343
161.581072	3098.086699	6.218061	-0.032111	3.059062
161.904564	3106.095636	6.223066	-0.032176	3.062774
162.146977	3114.125409	6.228070	-0.032227	3.066486
162.508780	3122.176692	6.233075	-0.032299	3.070209
163.151889	3130.246170	6.238080	-0.032424	3.073949
163.309896	3138.289773	6.243085	-0.032459	3.077651
163.369746	3146.319667	6.248090	-0.032476	3.081336
163.570257	3154.289149	6.253094	-0.032518	3.084997
163.876320	3162.352506	6.258099	-0.032581	3.088700
164.077639	3170.390404	6.263104	-0.032623	3.092383
164.307245	3178.452959	6.268109	-0.032672	3.096074
164.551392	3186.455292	6.273114	-0.032722	3.099733
164.831737	3194.471154	6.278118	-0.032780	3.103396
164.969033	3202.499870	6.283123	-0.032811	3.107055
165.289120	3210.538555	6.288128	-0.032876	3.110721
165.510877	3218.616595	6.293133	-0.032922	3.114397
165.626923	3226.620321	6.298138	-0.032949	3.118029
165.716634	3234.673997	6.303142	-0.032971	3.121679
166.095781	3242.646485	6.308147	-0.033047	3.125301
166.283508	3250.675583	6.313152	-0.033087	3.128936
166.469808	3258.760655	6.318157	-0.033127	3.132591
166.629406	3266.794797	6.323162	-0.033162	3.136218
166.716689	3274.805133	6.328166	-0.033184	3.139827
167.104046	3282.823290	6.333171	-0.033261	3.143449
167.131722	3290.853876	6.338176	-0.033272	3.147056
167.500200	3298.895444	6.343181	-0.033346	3.150679
167.833142	3306.977795	6.348186	-0.033413	3.154314
168.058211	3314.970472	6.353190	-0.033460	3.157900
168.402151	3322.997929	6.358195	-0.033530	3.161503
168.455433	3330.992035	6.363200	-0.033545	3.165074
168.687114	3339.022896	6.368205	-0.033593	3.168666
169.213363	3347.078231	6.373210	-0.033697	3.172276
169.280298	3355.116049	6.378214	-0.033714	3.175855
169.600211	3363.155691	6.383219	-0.033779	3.179442
169.866651	3371.140008	6.388224	-0.033834	3.182998
170.115894	3379.213226	6.393229	-0.033886	3.186588
170.191745	3387.271228	6.398234	-0.033905	3.190160
170.077071	3395.324577	6.403238	-0.033889	3.193718
170.441784	3403.367709	6.408243	-0.033963	3.197288
170.799730	3411.345647	6.413248	-0.034034	3.200824
171.017589	3419.340108	6.418253	-0.034080	3.204359
171.249534	3427.411692	6.423258	-0.034129	3.207923
171.186547	3435.473155	6.428262	-0.034122	3.211467
171.615302	3443.482587	6.433267	-0.034208	3.215005
171.752130	3451.495570	6.438272	-0.034238	3.218528
171.982326	3459.542906	6.443277	-0.034287	3.222066
172.323343	3467.529720	6.448282	-0.034355	3.225579
172.346934	3475.608395	6.453286	-0.034365	3.229114
172.925888	3483.661708	6.458291	-0.034478	3.232657
173.022605	3491.720024	6.463296	-0.034502	3.236179
173.044701	3499.698066	6.468301	-0.034511	3.239659
173.313021	3507.710108	6.473306	-0.034566	3.243160
173.633079	3515.738404	6.478310	-0.034631	3.246667
173.959097	3523.762782	6.483315	-0.034697	3.250168
174.074571	3531.795070	6.488320	-0.034724	3.253660
174.425088	3539.833351	6.493325	-0.034795	3.257160
174.702464	3547.833040	6.498330	-0.034851	3.260637
174.831134	3555.856352	6.503334	-0.034881	3.264115
175.293902	3563.889822	6.508339	-0.034972	3.267606
175.486379	3571.942802	6.513344	-0.035013	3.271092
175.713477	3579.991939	6.518349	-0.035061	3.274573
175.788283	3588.022871	6.523354	-0.035080	3.278037
175.967979	3596.026079	6.528358	-0.035119	3.281489
176.283802	3604.051763	6.533363	-0.035183	3.284953
176.638002	3612.078286	6.538368	-0.035254	3.288414
177.024635	3620.120017	6.543373	-0.035332	3.291880
177.054322	3628.186153	6.548378	-0.035343	3.295339
177.019429	3636.200141	6.553382	-0.035341	3.298770
177.440591	3644.211993	6.558387	-0.035425	3.302213
177.486538	3652.235620	6.563392	-0.035439	3.305643
177.631421	3660.301324	6.568397	-0.035471	3.309092
177.829126	3668.357686	6.573402	-0.035513	3.312535
178.016864	3676.364748	6.578406	-0.035554	3.315953
178.327831	3684.385520	6.583411	-0.035617	3.319378
178.213514	3692.396804	6.588416	-0.035601	3.322779
178.698016	3700.380934	6.593421	-0.035696	3.326188
178.960039	3708.399483	6.598426	-0.035750	3.329599
179.015376	3716.450233	6.603430	-0.035766	3.333013
179.445050	3724.511518	6.608435	-0.035851	3.336441
179.678901	3732.480064	6.613440	-0.035900	3.339820
179.910373	3740.518368	6.618445	-0.035949	3.343225
180.193830	3748.561992	6.623450	-0.036007	3.346630
180.366758	3756.578989	6.628454	-0.036044	3.350016
180.741985	3764.653606	6.633459	-0.036119	3.353431
180.744255	3772.700957	6.638464	-0.036125	3.356817
181.419669	3780.646290	6.643469	-0.036256	3.360181
181.462114	3788.697643	6.648474	-0.036269	3.363563
181.446381	3796.753876	6.653478	-0.036272	3.366942
181.769675	3804.796950	6.658483	-0.036337	3.370324
182.098768	3812.807485	6.663488	-0.036404	3.373689
182.060792	3820.875041	6.668493	-0.036402	3.377062
182.217374	3828.891680	6.673498	-0.036437	3.380417
182.585011	3836.885191	6.678502	-0.036510	3.383766
182.807091	3844.931196	6.683507	-0.036557	3.387129
182.895297	3852.954495	6.688512	-0.036579	3.390474
183.222327	3861.071710	6.693517	-0.036645	3.393864
183.545086	3869.069077	6.698522	-0.036710	3.397199
183.908123	3877.018479	6.703526	-0.036783	3.400513
184.043664	3885.047326	6.708531	-0.036814	3.403849
184.344479	3893.056921	6.713536	-0.036875	3.407180
184.546629	3901.078097	6.718541	-0.036918	3.410508
184.809261	3909.128673	6.723546	-0.036972	3.413847
184.830198	3917.153399	6.728550	-0.036982	3.417164
185.016951	3925.187521	6.733555	-0.037022	3.420488
185.065206	3933.225696	6.738560	-0.037036	3.423805
185.209701	3941.244920	6.743565	-0.037068	3.427114
185.548384	3949.273668	6.748570	-0.037137	3.430431
185.691833	3957.303368	6.753574	-0.037169	3.433738
185.927064	3965.357041	6.758579	-0.037218	3.437055
186.247164	3973.328071	6.763584	-0.037283	3.440337
186.309128	3981.364172	6.768589	-0.037299	3.443635
186.461294	3989.425943	6.773594	-0.037333	3.446942
186.767344	3997.406917	6.778598	-0.037395	3.450219
187.113694	4005.483317	6.783603	-0.037465	3.453533
187.212652	4013.526156	6.788608	-0.037489	3.456821
187.216227	4021.541418	6.793613	-0.037495	3.460092
187.557446	4029.549036	6.798618	-0.037564	3.463368
187.714800	4037.558217	6.803622	-0.037598	3.466636
187.878512	4045.599864	6.808627	-0.037634	3.469914
187.962976	4053.674632	6.813632	-0.037655	3.473199
188.330057	4061.711104	6.818637	-0.037729	3.476475
188.330900	4069.694679	6.823642	-0.037734	3.479715
188.508476	4077.697344	6.828646	-0.037773	3.482965
188.858042	4085.734295	6.833651	-0.037843	3.486231
189.053176	4093.709115	6.838656	-0.037885	3.489464
189.245437	4101.782821	6.843661	-0.037926	3.492734
189.550678	4109.811387	6.848666	-0.037988	3.495986
189.671149	4117.804525	6.853670	-0.038016	3.499216
189.874615	4125.842898	6.858675	-0.038059	3.502462
189.761207	4133.875108	6.863680	-0.038043	3.505694
190.117272	4141.896662	6.868685	-0.038115	3.508933
190.210969	4149.938027	6.873690	-0.038137	3.512168
190.650369	4157.926361	6.878694	-0.038225	3.515390
190.932133	4165.952089	6.883699	-0.038282	3.518619
191.010501	4173.994477	6.888704	-0.038302	3.521846
191.116037	4181.999345	6.893709	-0.038327	3.525055
191.527576	4190.013518	6.898714	-0.038409	3.528275
191.798919	4198.019166	6.903718	-0.038465	3.531484
192.023115	4206.107697	6.908723	-0.038512	3.534721
192.032448	4214.169703	6.913728	-0.038519	3.537939
192.529803	4222.160422	6.918733	-0.038617	3.541139
192.793128	4230.158733	6.923738	-0.038671	3.544333
192.891863	4238.186779	6.928742	-0.038695	3.547531
193.055628	4246.269164	6.933747	-0.038731	3.550750
193.253659	4254.378457	6.938752	-0.038773	3.553977
193.390692	4262.377720	6.943757	-0.038804	3.557156
193.781297	4270.343573	6.948762	-0.038882	3.560326
194.188665	4278.325736	6.953766	-0.038963	3.563500
194.349998	4286.369439	6.958771	-0.038998	3.566688
194.524524	4294.364175	6.963776	-0.039036	3.569855
194.774294	4302.410445	6.968781	-0.039088	3.573041
194.995637	4310.468448	6.973786	-0.039135	3.576228
195.176580	4318.429750	6.978790	-0.039174	3.579374
195.573882	4326.450754	6.983795	-0.039253	3.582546
195.564041	4334.478101	6.988800	-0.039256	3.585706
195.603993	4342.519294	6.993805	-0.039269	3.588870
195.789006	4350.582697	6.998810	-0.039309	3.592044
196.099198	4358.570446	7.003814	-0.039372	3.595189
196.368840	4366.586525	7.008819	-0.039427	3.598341
196.557444	4374.586010	7.013824	-0.039468	3.601482
196.933853	4382.565769	7.018829	-0.039543	3.604617
197.222815	4390.627453	7.023834	-0.039602	3.607780
197.144747	4398.663763	7.028838	-0.039593	3.610919
197.780088	4406.677143	7.033843	-0.039717	3.614067
197.825127	4414.728562	7.038848	-0.039730	3.617210
198.124958	4422.746065	7.043853	-0.039792	3.620344
198.199168	4430.771068	7.048858	-0.039811	3.623472
198.583476	4438.807286	7.053862	-0.039888	3.626610
198.754403	4446.819578	7.058867	-0.039925	3.629731
198.869418	4454.878063	7.063872	-0.039951	3.632865
199.121245	4462.931774	7.068877	-0.040004	3.635998
199.077476	4470.966859	7.073882	-0.040001	3.639114
199.260895	4478.957871	7.078886	-0.040040	3.642215
199.707443	4486.936289	7.083891	-0.040129	3.645317
199.766666	4494.965718	7.088896	-0.040145	3.648424
199.772861	4503.014498	7.093901	-0.040151	3.651536
200.203744	4511.052054	7.098906	-0.040237	3.654651
200.433003	4519.064079	7.103910	-0.040285	3.657749
200.600083	4527.079070	7.108915	-0.040321	3.660843
200.664291	4535.087525	7.113920	-0.040339	3.663930
200.970644	4543.146695	7.118925	-0.040401	3.667040
201.290987	4551.160757	7.123930	-0.040466	3.670130
201.389273	4559.178540	7.128934	-0.040490	3.673213
201.812133	4567.225621	7.133939	-0.040574	3.676314
201.880363	4575.189035	7.138944	-0.040592	3.679370
202.096989	4583.239828	7.143949	-0.040637	3.682461
202.232177	4591.223703	7.148954	-0.040668	3.685522
202.571480	4599.228725	7.153958	-0.040736	3.688593
202.838204	4607.318825	7.158963	-0.040791	3.691693
202.760370	4615.348243	7.163968	-0.040782	3.694758
203.187846	4623.371286	7.168973	-0.040867	3.697831
203.330298	4631.367966	7.173978	-0.040899	3.700884
203.533016	4639.346956	7.178982	-0.040942	3.703929
203.942577	4647.375971	7.183987	-0.041023	3.706996
204.051694	4655.405552	7.188992	-0.041049	3.710053
204.289937	4663.545352	7.193997	-0.041099	3.713152
204.384740	4671.626326	7.199002	-0.041122	3.716223
204.623936	4679.531224	7.204006	-0.041172	3.719229
205.067746	4687.558239	7.209011	-0.041259	3.722283
205.052156	4695.506323	7.214016	-0.041262	3.725293
205.363866	4703.573177	7.219021	-0.041325	3.728354
205.968261	4711.565763	7.224026	-0.041443	3.731391
205.959386	4719.597534	7.229030	-0.041447	3.734426
206.447456	4727.658768	7.234035	-0.041543	3.737481
206.564275	4735.609879	7.239040	-0.041570	3.740484
206.718787	4743.682766	7.244045	-0.041604	3.743530
206.979716	4751.706840	7.249050	-0.041658	3.746559
207.200853	4759.685194	7.254054	-0.041704	3.749566
207.539011	4767.774208	7.259059	-0.041773	3.752616
207.368201	4775.792054	7.264064	-0.041746	3.755625
207.802013	4783.793710	7.269069	-0.041832	3.758639
208.136111	4791.841324	7.274074	-0.041900	3.761665
208.264921	4799.802127	7.279078	-0.041929	3.764652
208.347192	4807.882192	7.284083	-0.041950	3.767680
208.710256	4815.876032	7.289088	-0.042023	3.770680
208.943220	4823.925935	7.294093	-0.042071	3.773695
208.937230	4832.005803	7.299098	-0.042076	3.776714
208.870125	4839.967763	7.304102	-0.042068	3.779684
209.204562	4848.026934	7.309107	-0.042136	3.782698
209.379514	4856.008233	7.314112	-0.042174	3.785677
209.629885	4864.009923	7.319117	-0.042226	3.788662
210.082806	4872.072491	7.324122	-0.042315	3.791673
210.067266	4880.103481	7.329126	-0.042318	3.794658
210.417254	4888.139724	7.334131	-0.042388	3.797652
210.677917	4896.090054	7.339136	-0.042442	3.800609
210.756744	4904.113607	7.344141	-0.042462	3.803587
211.128224	4912.154455	7.349146	-0.042537	3.806575
211.293792	4920.141080	7.354150	-0.042573	3.809537
211.725347	4928.188844	7.359155	-0.042658	3.812524
211.861859	4936.205867	7.364160	-0.042689	3.815492
211.936903	4944.217471	7.369165	-0.042708	3.818454
212.320155	4952.248358	7.374170	-0.042785	3.821427
212.222327	4960.249294	7.379174	-0.042772	3.824377
212.675060	4968.309326	7.384179	-0.042862	3.827357
212.761064	4976.310734	7.389184	-0.042883	3.830306
212.869087	4984.383313	7.394189	-0.042908	3.833280
212.880091	4992.405613	7.399194	-0.042916	3.836230
213.252392	5000.369048	7.404198	-0.042990	3.839164
213.428564	5008.409957	7.409203	-0.043029	3.842120
213.437306	5016.389741	7.414208	-0.043035	3.845049
213.933200	5024.453704	7.419213	-0.043133	3.848015
214.362831	5032.437366	7.424218	-0.043218	3.850948
214.603550	5040.487069	7.429222	-0.043269	3.853900
214.757988	5048.532363	7.434227	-0.043303	3.856846
214.962364	5056.523936	7.439232	-0.043346	3.859771
215.288224	5064.545059	7.444237	-0.043412	3.862707
215.499627	5072.564877	7.449242	-0.043457	3.865638
215.415323	5080.609246	7.454246	-0.043446	3.868570
215.872569	5088.652295	7.459251	-0.043537	3.871509
216.100347	5096.888817	7.464256	-0.043585	3.874513
216.145774	5104.859043	7.469261	-0.043598	3.877413
216.449679	5112.783004	7.474266	-0.043660	3.880300
216.581070	5120.721187	7.479270	-0.043690	3.883186
216.788314	5128.754297	7.484275	-0.043734	3.886106
216.905304	5136.750026	7.489280	-0.043761	3.889009
217.107869	5144.810251	7.494285	-0.043804	3.891934
217.295999	5152.832541	7.499290	-0.043844	3.894843
217.596724	5160.849084	7.504294	-0.043905	3.897750
217.757612	5168.847825	7.509299	-0.043941	3.900646
217.981133	5176.856303	7.514304	-0.043988	3.903544
218.273344	5184.880316	7.519309	-0.044047	3.906447
218.680983	5192.904583	7.524314	-0.044129	3.909350
218.849801	5200.913267	7.529318	-0.044165	3.912240
219.093937	5208.944974	7.534323	-0.044216	3.915138
219.368736	5216.973401	7.539328	-0.044273	3.918034
219.438966	5224.960797	7.544333	-0.044291	3.920909
219.499718	5232.991053	7.549338	-0.044308	3.923796
219.624882	5240.971906	7.554342	-0.044336	3.926665
219.924095	5249.016203	7.559347	-0.044397	3.929558
220.021423	5257.060802	7.564352	-0.044421	3.932446
220.098768	5265.066157	7.569357	-0.044440	3.935316
220.535815	5273.079066	7.574362	-0.044527	3.938194
220.356952	5281.073799	7.579366	-0.044499	3.941052
220.580495	5289.143029	7.584371	-0.044546	3.943942
220.915781	5297.128134	7.589376	-0.044614	3.946801
221.200499	5305.152214	7.594381	-0.044672	3.949672
221.227183	5313.245334	7.599386	-0.044682	3.952560
221.344322	5321.258641	7.604390	-0.044709	3.955419
221.809878	5329.240281	7.609395	-0.044801	3.958271
221.979739	5337.227785	7.614400	-0.044838	3.961118
221.999727	5345.243070	7.619405	-0.044847	3.963971
222.293600	5353.263642	7.624410	-0.044907	3.966827
222.470225	5361.264818	7.629414	-0.044946	3.969673
222.793529	5369.327478	7.634419	-0.045011	3.972541
222.690351	5377.322477	7.639424	-0.044997	3.975376
222.886471	5385.382511	7.644429	-0.045039	3.978236
223.088523	5393.394391	7.649434	-0.045082	3.981078
223.286580	5401.387570	7.654438	-0.045124	3.983911
223.573769	5409.438988	7.659443	-0.045183	3.986764
223.714464	5417.458745	7.664448	-0.045214	3.989601
224.027955	5425.488002	7.669453	-0.045278	3.992442
224.320478	5433.557679	7.674458	-0.045338	3.995296
224.461506	5441.556784	7.679462	-0.045369	3.998119
224.654249	5449.548683	7.684467	-0.045411	4.000940
224.836557	5457.565391	7.689472	-0.045450	4.003766
225.201846	5465.563831	7.694477	-0.045523	4.006587
225.508452	5473.614147	7.699482	-0.045586	4.009424
225.536980	5481.652211	7.704486	-0.045596	4.012249
225.838435	5489.692122	7.709491	-0.045658	4.015078
226.064283	5497.686825	7.714496	-0.045705	4.017887
226.083622	5505.722820	7.719501	-0.045714	4.020706
226.433702	5513.725364	7.724506	-0.045784	4.023516
226.571470	5521.720411	7.729510	-0.045815	4.026319
226.765545	5529.750829	7.734515	-0.045857	4.029132
226.734196	5537.777714	7.739520	-0.045856	4.031939
227.295819	5545.864801	7.744525	-0.045966	4.034774
227.408074	5553.896134	7.749530	-0.045992	4.037581
227.829914	5561.777949	7.754534	-0.046076	4.040338
228.118046	5569.806977	7.759539	-0.046135	4.043142
228.230518	5577.821172	7.764544	-0.046161	4.045937
228.271877	5585.838502	7.769549	-0.046174	4.048730
228.664458	5593.913452	7.774554	-0.046253	4.051546
228.772517	5601.908777	7.779558	-0.046278	4.054328
228.958033	5609.959531	7.784563	-0.046318	4.057129
229.138992	5617.919904	7.789568	-0.046357	4.059896
229.564173	5625.939896	7.794573	-0.046442	4.062686
229.840784	5633.959803	7.799578	-0.046498	4.065471
229.852224	5641.992244	7.804582	-0.046506	4.068256
230.134540	5650.021316	7.809587	-0.046564	4.071040
230.360704	5658.045584	7.814592	-0.046611	4.073821
230.577205	5666.068590	7.819597	-0.046657	4.076599
230.734433	5674.065137	7.824602	-0.046691	4.079365
230.941363	5682.067974	7.829606	-0.046735	4.082132
231.092132	5690.061306	7.834611	-0.046768	4.084893
231.071338	5698.126440	7.839616	-0.046770	4.087675
231.401528	5706.100347	7.844621	-0.046837	4.090428
231.641640	5714.196514	7.849626	-0.046887	4.093220
231.669935	5722.181098	7.854630	-0.046897	4.095969
231.957550	5730.215816	7.859635	-0.046956	4.098736
232.225024	5738.241399	7.864640	-0.047011	4.101499
232.491268	5746.221647	7.869645	-0.047066	4.104243
232.637257	5754.285482	7.874650	-0.047099	4.107014
232.724658	5762.239547	7.879654	-0.047120	4.109743
233.004315	5770.332211	7.884659	-0.047178	4.112521
232.994931	5778.356191	7.889664	-0.047181	4.115270
233.297062	5786.375202	7.894669	-0.047243	4.118020
233.588508	5794.340757	7.899674	-0.047302	4.120749
233.648446	5802.349220	7.904678	-0.047319	4.123487
233.762019	5810.393126	7.909683	-0.047345	4.126237
234.061377	5818.373693	7.914688	-0.047406	4.128966
234.130975	5826.466591	7.919693	-0.047425	4.131728
234.506296	5834.510299	7.924698	-0.047500	4.134476
234.667884	5842.503710	7.929702	-0.047535	4.137202
234.917343	5850.496681	7.934707	-0.047587	4.139926
235.151997	5858.565282	7.939712	-0.047636	4.142675
235.334176	5866.536453	7.944717	-0.047675	4.145388
235.336055	5874.590725	7.949722	-0.047681	4.148125
235.479179	5882.605099	7.954726	-0.047713	4.150849
235.911481	5890.656506	7.959731	-0.047799	4.153587
236.107416	5898.634747	7.964736	-0.047840	4.156295
236.229166	5906.632719	7.969741	-0.047868	4.159007
236.455924	5914.704421	7.974746	-0.047916	4.161744
236.623845	5922.624785	7.979750	-0.047952	4.164427
236.983069	5930.701962	7.984755	-0.048025	4.167164
237.048955	5938.710040	7.989760	-0.048042	4.169872
237.089009	5946.733434	7.994765	-0.048055	4.172583
237.525052	5954.786403	7.999770	-0.048141	4.175306
237.478897	5962.769440	8.004774	-0.048138	4.178000
237.702187	5970.806527	8.009779	-0.048185	4.180712
237.803354	5978.786966	8.014784	-0.048209	4.183402
238.112323	5986.798565	8.019789	-0.048272	4.186103
238.340817	5994.845810	8.024794	-0.048320	4.188814
238.315155	6002.842126	8.029798	-0.048320	4.191503
238.753528	6011.007778	8.034803	-0.048407	4.194252
238.859002	6018.978031	8.039808	-0.048432	4.196930
238.967332	6026.917982	8.044813	-0.048458	4.199596
239.299099	6034.957805	8.049818	-0.048525	4.202296
239.322725	6042.899407	8.054822	-0.048534	4.204959
239.330817	6050.960250	8.059827	-0.048541	4.207659
239.518180	6058.917463	8.064832	-0.048581	4.210325
239.841168	6066.965446	8.069837	-0.048647	4.213021
240.007099	6074.990596	8.074842	-0.048683	4.215706
240.122325	6082.981277	8.079846	-0.048710	4.218377
240.300429	6091.038871	8.084851	-0.048748	4.221069
240.386294	6099.020091	8.089856	-0.048770	4.223734
240.684543	6107.055641	8.094861	-0.048830	4.226416
240.902408	6115.093060	8.099866	-0.048876	4.229097
241.120262	6123.096298	8.104870	-0.048922	4.231765
241.203457	6131.166576	8.109875	-0.048943	4.234452
241.545532	6139.180462	8.114880	-0.049012	4.237121
241.799206	6147.099564	8.119885	-0.049064	4.239756
241.815040	6155.208743	8.124890	-0.049073	4.242450
242.052591	6163.138418	8.129894	-0.049122	4.245085
242.401211	6171.243339	8.134899	-0.049193	4.247778
242.567423	6179.210524	8.139904	-0.049229	4.250421
242.694348	6187.242204	8.144909	-0.049258	4.253084
242.863009	6195.295805	8.149914	-0.049294	4.255753
243.064011	6203.270666	8.154918	-0.049337	4.258394
243.263177	6211.306321	8.159923	-0.049380	4.261054
243.361588	6219.318478	8.164928	-0.049403	4.263703
243.875539	6227.327987	8.169933	-0.049504	4.266353
244.075433	6235.402607	8.174938	-0.049547	4.269021
244.110704	6243.400332	8.179942	-0.049559	4.271660
244.391513	6251.463257	8.184947	-0.049616	4.274320
244.671511	6259.473536	8.189952	-0.049674	4.276962
244.869503	6267.433038	8.194957	-0.049716	4.279585
244.969122	6275.481490	8.199962	-0.049740	4.282235
245.120417	6283.429293	8.204966	-0.049773	4.284850
245.219780	6291.468762	8.209971	-0.049797	4.287493
245.422238	6299.499405	8.214976	-0.049840	4.290133
245.744765	6307.529428	8.219981	-0.049905	4.292772
245.900227	6315.618847	8.224986	-0.049940	4.295427
245.644586	6323.625626	8.229990	-0.049897	4.298051
245.962056	6331.581276	8.234995	-0.049962	4.300660
246.094939	6339.639511	8.240000	-0.049992	4.303300
246.390213	6347.581760	8.245005	-0.050052	4.305901
246.562462	6355.628098	8.250010	-0.050089	4.308535
246.549839	6363.656747	8.255014	-0.050092	4.311159
246.795918	6371.709513	8.260019	-0.050143	4.313791
246.845892	6379.742841	8.265024	-0.050158	4.316414
247.182946	6387.686891	8.270029	-0.050226	4.319009
247.466530	6395.735638	8.275034	-0.050284	4.321635
247.355672	6403.701852	8.280038	-0.050269	4.324231
247.445046	6411.773169	8.285043	-0.050291	4.326860
247.744484	6419.760682	8.290048	-0.050352	4.329462
247.895425	6427.794560	8.295053	-0.050385	4.332076
248.175256	6435.845165	8.300058	-0.050443	4.334695
248.322321	6443.878425	8.305062	-0.050475	4.337306
248.519125	6451.832893	8.310067	-0.050517	4.339890
248.495562	6459.835968	8.315072	-0.050518	4.342487
248.888084	6467.853087	8.320077	-0.050597	4.345090
249.054856	6475.899751	8.325082	-0.050633	4.347699
249.013568	6483.907076	8.330086	-0.050631	4.350292
249.407584	6491.968859	8.335091	-0.050709	4.352904
249.709357	6500.022890	8.340096	-0.050771	4.355512
249.822583	6508.001322	8.345101	-0.050797	4.358092
249.978477	6515.997288	8.350106	-0.050832	4.360677
250.114244	6523.957817	8.355110	-0.050862	4.363249
250.431099	6531.999216	8.360115	-0.050926	4.365846
250.446640	6539.997606	8.365120	-0.050935	4.368426
250.741573	6547.999739	8.370125	-0.050995	4.371007
251.252481	6556.085398	8.375130	-0.051095	4.373615
251.164656	6564.095133	8.380134	-0.051084	4.376193
251.534749	6572.075643	8.385139	-0.051158	4.378763
251.595217	6580.104999	8.390144	-0.051175	4.381346
251.925260	6588.090963	8.395149	-0.051242	4.383914
252.246529	6596.136338	8.400154	-0.051307	4.386500
252.277602	6604.105654	8.405158	-0.051318	4.389059
252.475171	6612.186016	8.410163	-0.051360	4.391652
252.373951	6620.220410	8.415168	-0.051347	4.394228
252.616019	6628.236630	8.420173	-0.051397	4.396798
252.989351	6636.227361	8.425178	-0.051472	4.399359
253.044537	6644.223803	8.430182	-0.051487	4.401919
253.353537	6652.233840	8.435187	-0.051550	4.404482
253.532927	6660.298446	8.440192	-0.051589	4.407062
253.877411	6668.267723	8.445197	-0.051658	4.409609
254.025174	6676.341387	8.450202	-0.051691	4.412188
254.247216	6684.330725	8.455206	-0.051738	4.414739
254.498340	6692.401727	8.460211	-0.051790	4.417314
254.545686	6700.362776	8.465216	-0.051804	4.419852
254.527068	6708.427346	8.470221	-0.051806	4.422421
254.961911	6716.381694	8.475226	-0.051892	4.424956
254.999367	6724.436288	8.480230	-0.051904	4.427519
255.236178	6732.412473	8.485235	-0.051954	4.430056
255.616327	6740.506469	8.490240	-0.052030	4.432630
255.786993	6748.518489	8.495245	-0.052067	4.435176
255.899071	6756.570342	8.500250	-0.052093	4.437733
256.050393	6764.458103	8.505254	-0.052126	4.440236
256.416995	6772.575310	8.510259	-0.052200	4.442811
256.576142	6780.517516	8.515264	-0.052235	4.445329
256.497827	6788.564649	8.520269	-0.052226	4.447877
256.781953	6796.570825	8.525274	-0.052284	4.450413
256.903761	6804.597318	8.530278	-0.052312	4.452952
257.132555	6812.618388	8.535283	-0.052360	4.455489
257.168947	6820.640271	8.540288	-0.052372	4.458024
257.182589	6828.642261	8.545293	-0.052380	4.460552
257.322783	6836.685088	8.550298	-0.052411	4.463091
257.598290	6844.631198	8.555302	-0.052468	4.465598
257.810955	6852.702369	8.560307	-0.052513	4.468144
258.018276	6860.705940	8.565312	-0.052557	4.470666
258.336202	6868.718020	8.570317	-0.052621	4.473191
258.478903	6876.800898	8.575322	-0.052653	4.475735
258.541548	6884.791884	8.580327	-0.052670	4.478249
258.702105	6892.795453	8.585331	-0.052705	4.480765
258.866956	6900.769762	8.590336	-0.052741	4.483271
259.058277	6908.756334	8.595341	-0.052782	4.485780
259.160028	6916.854681	8.600346	-0.052806	4.488322
259.229256	6924.813574	8.605351	-0.052824	4.490819
259.630217	6932.874885	8.610355	-0.052904	4.493347
259.816662	6940.899721	8.615360	-0.052944	4.495862
259.881197	6948.882191	8.620365	-0.052962	4.498361
260.222820	6956.912979	8.625370	-0.053031	4.500876
260.290862	6964.911440	8.630375	-0.053049	4.503377
260.530096	6972.914180	8.635379	-0.053099	4.505880
260.783344	6980.947363	8.640384	-0.053151	4.508390
260.990506	6988.951434	8.645389	-0.053195	4.510890
261.135329	6997.086519	8.650394	-0.053227	4.513429
261.321708	7005.077812	8.655399	-0.053267	4.515922
261.746628	7013.060140	8.660403	-0.053352	4.518411
261.761002	7020.980283	8.665408	-0.053360	4.520879
261.801166	7029.016945	8.670413	-0.053372	4.523381
262.098291	7037.051662	8.675418	-0.053433	4.525882
262.138943	7045.024026	8.680423	-0.053446	4.528362
262.317529	7053.093509	8.685427	-0.053484	4.530871
262.306725	7061.141327	8.690432	-0.053488	4.533371
262.548238	7069.113971	8.695437	-0.053538	4.535848
262.888279	7077.170127	8.700442	-0.053607	4.538348
263.103094	7085.113609	8.705447	-0.053652	4.540812
263.436083	7093.133546	8.710451	-0.053719	4.543299
263.575633	7101.128529	8.715456	-0.053750	4.545776
263.688407	7109.146188	8.720461	-0.053777	4.548259
263.786302	7117.193557	8.725466	-0.053800	4.550750
264.032951	7125.225711	8.730471	-0.053852	4.553235
264.076305	7133.279149	8.735475	-0.053865	4.555725
264.238774	7141.342736	8.740480	-0.053900	4.558216
264.576949	7149.243480	8.745485	-0.053969	4.560657
264.635821	7157.302074	8.750490	-0.053985	4.563144
264.732356	7165.236442	8.755495	-0.054008	4.565592
265.058693	7173.330613	8.760499	-0.054074	4.568087
265.217045	7181.335418	8.765504	-0.054109	4.570554
265.232488	7189.406718	8.770509	-0.054117	4.573040
265.505088	7197.404926	8.775514	-0.054173	4.575502
265.732767	7205.445176	8.780519	-0.054221	4.577975
265.873184	7213.394498	8.785523	-0.054252	4.580419
266.091516	7221.411062	8.790528	-0.054298	4.582883
266.297203	7229.387304	8.795533	-0.054342	4.585333
266.690632	7237.474618	8.800538	-0.054421	4.587815
266.533229	7245.445537	8.805543	-0.054397	4.590261
266.828825	7253.565202	8.810547	-0.054457	4.592751
267.055862	7261.572213	8.815552	-0.054505	4.595205
267.153855	7269.598861	8.820557	-0.054528	4.597663
267.394613	7277.540149	8.825562	-0.054578	4.600094
267.471328	7285.568305	8.830567	-0.054598	4.602551
267.634957	7293.509977	8.835571	-0.054634	4.604979
267.739904	7301.600936	8.840576	-0.054658	4.607452
267.991061	7309.527796	8.845581	-0.054710	4.609874
268.172505	7317.649074	8.850586	-0.054750	4.612353
268.189796	7325.641498	8.855591	-0.054758	4.614792
268.533517	7333.694050	8.860595	-0.054827	4.617248
268.645919	7341.668608	8.865600	-0.054854	4.619679
268.805930	7349.700824	8.870605	-0.054889	4.622126
269.274857	7357.684783	8.875610	-0.054981	4.624556
269.456415	7365.706246	8.880615	-0.055020	4.626998
269.483190	7373.728511	8.885619	-0.055031	4.629438
269.534813	7381.755101	8.890624	-0.055046	4.631878
269.795257	7389.768120	8.895629	-0.055099	4.634312
270.002926	7397.829500	8.900634	-0.055143	4.636760
270.050014	7405.774280	8.905639	-0.055157	4.639172
270.286293	7413.835108	8.910643	-0.055207	4.641617
270.553351	7421.785059	8.915648	-0.055262	4.644027
270.629386	7429.835316	8.920653	-0.055281	4.646467
270.882754	7437.856595	8.925658	-0.055334	4.648896
270.940587	7445.875093	8.930663	-0.055350	4.651323
271.281214	7453.913608	8.935667	-0.055419	4.653755
271.431570	7461.904925	8.940672	-0.055452	4.656171
271.497122	7469.911387	8.945677	-0.055469	4.658591
271.807089	7477.959535	8.950682	-0.055532	4.661022
271.897198	7485.933222	8.955687	-0.055554	4.663429
272.101692	7493.981063	8.960691	-0.055598	4.665858
272.408324	7501.971671	8.965696	-0.055660	4.668267
272.549626	7509.974841	8.970701	-0.055692	4.670680
272.574423	7518.075788	8.975706	-0.055702	4.673120
272.801744	7526.113873	8.980711	-0.055749	4.675541
273.052528	7534.102427	8.985715	-0.055801	4.677945
273.161274	7542.043344	8.990720	-0.055827	4.680333
273.341242	7550.025227	8.995725	-0.055866	4.682733
273.658455	7558.046579	9.000730	-0.055930	4.685143
273.725933	7566.064076	9.005735	-0.055948	4.687551
273.902666	7574.049124	9.010739	-0.055986	4.689947
274.056325	7582.167206	9.015744	-0.056020	4.692383
274.177919	7590.142490	9.020749	-0.056048	4.694774
274.414896	7598.206202	9.025754	-0.056098	4.697191
274.493994	7606.099788	9.030759	-0.056117	4.699555
274.803745	7614.217363	9.035763	-0.056181	4.701985
274.876878	7622.153513	9.040768	-0.056199	4.704360
274.892279	7630.162087	9.045773	-0.056208	4.706756
275.287369	7638.238865	9.050778	-0.056286	4.709169
275.305201	7646.233809	9.055783	-0.056295	4.711558
275.407158	7654.273373	9.060787	-0.056319	4.713959
275.642671	7662.298526	9.065792	-0.056369	4.716354
275.975952	7670.264997	9.070797	-0.056436	4.718730
276.231301	7678.289273	9.075802	-0.056489	4.721122
276.145323	7686.295293	9.080807	-0.056478	4.723508
276.307605	7694.329998	9.085811	-0.056514	4.725901
276.525576	7702.382037	9.090816	-0.056559	4.728298
276.613322	7710.394841	9.095821	-0.056581	4.730682
276.825430	7718.460374	9.100826	-0.056626	4.733081
276.816198	7726.425662	9.105831	-0.056629	4.735449
277.045993	7734.490210	9.110835	-0.056678	4.737844
277.140395	7742.450082	9.115840	-0.056700	4.740208
277.323939	7750.458176	9.120845	-0.056740	4.742584
277.533582	7758.457003	9.125850	-0.056784	4.744957
277.741686	7766.498867	9.130855	-0.056828	4.747341
278.150209	7774.540019	9.135859	-0.056910	4.749723
278.275685	7782.529034	9.140864	-0.056938	4.752089
278.417464	7790.598237	9.145869	-0.056970	4.754477
278.520176	7798.586627	9.150874	-0.056995	4.756841
278.593718	7806.540640	9.155879	-0.057013	4.759193
278.556159	7814.582669	9.160883	-0.057012	4.761571
278.857712	7822.557306	9.165888	-0.057073	4.763926
279.098228	7830.575338	9.170893	-0.057123	4.766294
279.252264	7838.585648	9.175898	-0.057157	4.768657
279.237014	7846.638841	9.180903	-0.057160	4.771034
279.579514	7854.688567	9.185907	-0.057229	4.773406
279.648215	7862.738386	9.190912	-0.057247	4.775778
279.675918	7870.667610	9.195917	-0.057257	4.778114
280.084073	7878.724228	9.200922	-0.057339	4.780485
280.393991	7886.651930	9.205927	-0.057402	4.782817
280.389026	7894.723094	9.210931	-0.057406	4.785191
280.315126	7902.758950	9.215936	-0.057398	4.787554
280.717065	7910.720285	9.220941	-0.057478	4.789892
280.859845	7918.787795	9.225946	-0.057510	4.792261
280.976084	7926.796170	9.230951	-0.057537	4.794611
281.211367	7934.879673	9.235955	-0.057586	4.796982
281.317456	7942.786232	9.240960	-0.057611	4.799301
281.604913	7950.813721	9.245965	-0.057670	4.801652
281.894136	7958.815453	9.250970	-0.057729	4.803995
281.791259	7966.836799	9.255975	-0.057715	4.806345
281.964437	7974.857282	9.260979	-0.057752	4.808692
282.211071	7982.931092	9.265984	-0.057804	4.811053
282.498667	7990.319857	9.270989	-0.057862	4.813212
282.586541	7994.912818	9.275994	-0.057882	4.814554

282.616340	7997.198318	9.280999	-0.057889	4.815222
282.800059	7998.643938	9.286003	-0.057924	4.815643
282.976699	7999.282867	9.291008	-0.057957	4.815829
282.875564	7999.815273	9.296013	-0.057939	4.815985
283.143617	7999.830835	9.301018	-0.057989	4.815988
283.066110	7999.862558	9.306023	-0.057975	4.815998
283.014923	7999.814622	9.311027	-0.057965	4.815984
283.132887	7999.807156	9.316032	-0.057987	4.815981
283.186656	7999.795319	9.321037	-0.057997	4.815978
283.130327	7999.846659	9.326042	-0.057987	4.815993
283.217750	7999.725379	9.331047	-0.058003	4.815957
283.523739	7999.815356	9.336051	-0.058060	4.815982
283.549750	7999.799809	9.341056	-0.058065	4.815977
283.440418	7999.822406	9.346061	-0.058045	4.815984
283.561781	7999.906893	9.351066	-0.058068	4.816008
283.634800	7999.844117	9.356071	-0.058081	4.815990
283.710120	7999.902125	9.361075	-0.058095	4.816006
283.792158	7999.897212	9.366080	-0.058111	4.816004
284.038127	7999.815140	9.371085	-0.058157	4.815979
283.966298	7999.916420	9.376090	-0.058143	4.816009
283.738032	7999.884498	9.381095	-0.058101	4.816001
283.878631	7999.922322	9.386099	-0.058127	4.816011
284.094703	7999.879242	9.391104	-0.058167	4.815997
283.918745	7999.872846	9.396109	-0.058135	4.815996
284.303882	7999.872373	9.401114	-0.058207	4.815994
284.265898	7999.869554	9.406119	-0.058200	4.815994
284.276816	7999.847321	9.411123	-0.058202	4.815987
284.232088	7999.907422	9.416128	-0.058193	4.816005
284.190227	7999.814776	9.421133	-0.058186	4.815978
284.235040	7999.824146	9.426138	-0.058194	4.815981
284.209761	7999.903833	9.431143	-0.058190	4.816004
284.314583	7999.871554	9.436147	-0.058209	4.815994
284.662004	7999.890698	9.441152	-0.058274	4.815998
284.368681	7999.845839	9.446157	-0.058219	4.815986
284.548295	7999.844837	9.451162	-0.058253	4.815985
284.566858	7999.816332	9.456167	-0.058256	4.815976
284.623111	7999.895365	9.461171	-0.058267	4.815999
284.389109	7999.938135	9.466176	-0.058224	4.816013
284.428738	7999.901464	9.471181	-0.058231	4.816002
284.693008	7999.920167	9.476186	-0.058280	4.816006
284.449994	7999.947813	9.481191	-0.058235	4.816015
284.601101	7999.947362	9.486195	-0.058263	4.816015
284.795212	7999.920979	9.491200	-0.058300	4.816006
284.730234	7999.838597	9.496205	-0.058287	4.815982
284.759632	7999.925691	9.501210	-0.058293	4.816007
284.886609	7999.851072	9.506215	-0.058317	4.815985
284.874848	7999.878648	9.511219	-0.058315	4.815993
284.890275	7999.952666	9.516224	-0.058318	4.816015
284.941165	7999.917268	9.521229	-0.058327	4.816004
285.065582	7999.907784	9.526234	-0.058350	4.816000
284.334124	7999.951127	9.531239	-0.058214	4.816017
284.735350	7999.987279	9.536243	-0.058289	4.816025
284.824465	8000.003866	9.541248	-0.058306	4.816030
284.621554	7999.965992	9.546253	-0.058268	4.816020
284.903001	7999.972185	9.551258	-0.058321	4.816020
284.670410	7999.971170	9.556263	-0.058277	4.816021
284.868409	7999.949132	9.561267	-0.058314	4.816014
284.912870	7999.916823	9.566272	-0.058323	4.816004
284.911430	7999.854829	9.571277	-0.058322	4.815986
285.274884	7999.926626	9.576282	-0.058390	4.816005
285.019965	7999.852544	9.581287	-0.058343	4.815985
285.130034	7999.900500	9.586291	-0.058363	4.815998
285.197813	7999.904946	9.591296	-0.058376	4.815999
285.191370	7999.895219	9.596301	-0.058375	4.815996
285.250591	7999.897372	9.601306	-0.058386	4.815996
285.287593	7999.877750	9.606311	-0.058393	4.815990
285.445317	7999.903066	9.611315	-0.058422	4.815997
285.428145	7999.897418	9.616320	-0.058419	4.815995
285.416709	7999.899355	9.621325	-0.058417	4.815996
285.438465	7999.961735	9.626330	-0.058421	4.816014
285.356025	7999.905747	9.631335	-0.058406	4.815998
285.522024	7999.917322	9.636339	-0.058437	4.816001
285.499784	7999.922268	9.641344	-0.058433	4.816002
285.256067	7999.888993	9.646349	-0.058388	4.815994
285.221717	7999.925776	9.651354	-0.058381	4.816005
285.425767	7999.903848	9.656359	-0.058420	4.815997
285.636525	7999.882043	9.661363	-0.058459	4.815990
285.345994	7999.967595	9.666368	-0.058405	4.816016
285.204653	7999.951141	9.671373	-0.058379	4.816012
285.351977	7999.931388	9.676378	-0.058406	4.816006
285.350129	7999.873661	9.681383	-0.058406	4.815989
285.472076	7999.858789	9.686387	-0.058429	4.815984
285.690774	7999.933298	9.691392	-0.058469	4.816005
285.361880	7999.931599	9.696397	-0.058408	4.816006
285.366859	7999.952000	9.701402	-0.058409	4.816012
285.285370	7999.938772	9.706407	-0.058394	4.816008
285.627095	7999.916143	9.711411	-0.058458	4.816000
285.515286	7999.957928	9.716416	-0.058437	4.816013
285.151659	7999.976969	9.721421	-0.058370	4.816020
285.509641	7999.972801	9.726426	-0.058436	4.816017
285.336209	7999.955764	9.731431	-0.058404	4.816013
285.573578	7999.920551	9.736435	-0.058448	4.816001
285.466312	7999.966693	9.741440	-0.058428	4.816015
285.522235	7999.900399	9.746445	-0.058439	4.815996
285.692755	8000.012501	9.751450	-0.058471	4.816028
285.738454	7999.903278	9.756455	-0.058479	4.815995
285.944050	7999.873899	9.761459	-0.058518	4.815986
285.528704	7999.916576	9.766464	-0.058440	4.816000
285.488370	7999.881656	9.771469	-0.058433	4.815990
285.543223	7999.956392	9.776474	-0.058443	4.816012
285.804203	7999.844672	9.781479	-0.058492	4.815978
285.769213	7999.862209	9.786483	-0.058486	4.815983
285.872216	7999.892942	9.791488	-0.058505	4.815992
285.863434	7999.892790	9.796493	-0.058503	4.815992
285.870845	7999.974143	9.801498	-0.058505	4.816015
285.430604	7999.906305	9.806503	-0.058423	4.815998
285.687598	7999.907781	9.811507	-0.058471	4.815997
285.781765	7999.888130	9.816512	-0.058488	4.815991
285.812574	7999.864121	9.821517	-0.058494	4.815984
285.872581	7999.978488	9.826522	-0.058505	4.816017
285.851190	7999.927884	9.831527	-0.058502	4.816002
285.772594	7999.941422	9.836531	-0.058487	4.816006
285.804013	7999.960167	9.841536	-0.058493	4.816012
285.687993	7999.939899	9.846541	-0.058471	4.816006
285.797287	8000.022037	9.851546	-0.058492	4.816030
285.866634	7999.930341	9.856551	-0.058505	4.816003
285.819276	8000.023521	9.861555	-0.058496	4.816030
285.867988	7999.974192	9.866560	-0.058505	4.816015
285.974048	7999.962237	9.871565	-0.058525	4.816011
286.142434	7999.935388	9.876570	-0.058556	4.816003
286.187733	7999.910574	9.881575	-0.058565	4.815995
286.197958	7999.861613	9.886579	-0.058567	4.815981
286.033624	7999.932363	9.891584	-0.058536	4.816002
286.202242	7999.884146	9.896589	-0.058568	4.815987
286.138560	7999.970619	9.901594	-0.058556	4.816013
285.950222	7999.945830	9.906599	-0.058521	4.816007
286.116576	7999.908257	9.911603	-0.058552	4.815995
286.283345	7999.961522	9.916608	-0.058583	4.816010
286.126458	7999.888150	9.921613	-0.058554	4.815989
286.141455	7999.972848	9.926618	-0.058557	4.816014
286.182630	7999.906284	9.931623	-0.058565	4.815994
286.271356	7999.929277	9.936627	-0.058581	4.816000
286.055152	7999.984124	9.941632	-0.058541	4.816017
286.067354	7999.917033	9.946637	-0.058544	4.815998
286.104258	7999.925192	9.951642	-0.058551	4.816000
286.031100	7999.829835	9.956647	-0.058537	4.815972
286.141775	7999.861776	9.961651	-0.058558	4.815981
286.127255	7999.876479	9.966656	-0.058555	4.815985
286.032694	7999.818133	9.971661	-0.058537	4.815969
286.180928	7999.950134	9.976666	-0.058565	4.816007
286.214977	7999.883441	9.981671	-0.058572	4.815987
286.222482	7999.848322	9.986675	-0.058573	4.815977
286.248466	7999.930014	9.991680	-0.058578	4.816000
286.293923	7999.890243	9.996685	-0.058587	4.815989
286.647328	7999.891337	10.001690	-0.058652	4.815987
286.405164	7999.878390	10.006695	-0.058607	4.815985
286.630509	7999.835480	10.011699	-0.058649	4.815971
286.539177	7999.864815	10.016704	-0.058633	4.815980
286.509670	7999.842914	10.021709	-0.058627	4.815974
286.467427	7999.896651	10.026714	-0.058619	4.815990
286.498797	7999.899367	10.031719	-0.058625	4.815990
286.526937	7999.874240	10.036723	-0.058631	4.815983
286.560654	7999.925085	10.041728	-0.058637	4.815997
286.455749	7999.895401	10.046733	-0.058617	4.815989
286.513910	7999.885781	10.051738	-0.058628	4.815986
286.244913	7999.844564	10.056743	-0.058578	4.815976
286.491571	7999.902488	10.061747	-0.058624	4.815991
286.560073	7999.880233	10.066752	-0.058637	4.815984
286.250369	7999.829727	10.071757	-0.058580	4.815971
286.409995	7999.910644	10.076762	-0.058609	4.815994
286.481951	7999.904481	10.081767	-0.058623	4.815992
286.603407	7999.872503	10.086771	-0.058646	4.815982
286.435604	7999.879076	10.091776	-0.058614	4.815985
286.373994	7999.859797	10.096781	-0.058603	4.815979
286.620109	7999.915574	10.101786	-0.058649	4.815994
286.460607	7999.923366	10.106791	-0.058619	4.815997
286.616658	7999.880263	10.111795	-0.058648	4.815984
286.621992	7999.926317	10.116800	-0.058650	4.815997
286.693637	7999.874199	10.121805	-0.058663	4.815982
286.571783	7999.874127	10.126810	-0.058640	4.815982
286.440857	7999.838627	10.131815	-0.058616	4.815973
286.508019	7999.854817	10.136819	-0.058629	4.815977
286.506041	7999.864406	10.141824	-0.058628	4.815980
286.415884	7999.872391	10.146829	-0.058612	4.815983
286.438475	7999.876015	10.151834	-0.058616	4.815984
286.460174	7999.894583	10.156839	-0.058620	4.815989
286.391813	7999.888005	10.161843	-0.058607	4.815987
286.663740	7999.934634	10.166848	-0.058658	4.816000
286.723934	7999.875896	10.171853	-0.058669	4.815982
286.679273	7999.909286	10.176858	-0.058661	4.815992
286.511620	7999.873118	10.181863	-0.058630	4.815982
286.802374	7999.869866	10.186867	-0.058684	4.815980
286.725294	7999.936861	10.191872	-0.058670	4.816000
286.565413	7999.843130	10.196877	-0.058640	4.815973
286.958824	7999.903725	10.201882	-0.058714	4.815989
286.884113	7999.907716	10.206887	-0.058700	4.815990
286.684282	7999.955381	10.211891	-0.058663	4.816005
286.704148	7999.988876	10.216896	-0.058666	4.816015
286.602922	7999.881252	10.221901	-0.058648	4.815984
286.688665	7999.948003	10.226906	-0.058664	4.816003
286.710716	7999.940932	10.231911	-0.058668	4.816001
286.818509	7999.875580	10.236915	-0.058688	4.815981
286.837031	7999.926148	10.241920	-0.058692	4.815996
286.663674	7999.932619	10.246925	-0.058659	4.815999
286.678245	7999.929686	10.251930	-0.058662	4.815998
286.713365	7999.953842	10.256935	-0.058669	4.816005
286.613261	7999.914628	10.261939	-0.058650	4.815994
286.702005	7999.932279	10.266944	-0.058667	4.815999
286.667577	7999.931661	10.271949	-0.058661	4.815999
286.846659	7999.970190	10.276954	-0.058694	4.816009
286.691796	7999.932117	10.281959	-0.058665	4.815999
286.867094	7999.906462	10.286963	-0.058698	4.815990
286.745626	7999.938454	10.291968	-0.058675	4.816000
286.772123	7999.881240	10.296973	-0.058680	4.815983
286.919828	7999.961943	10.301978	-0.058708	4.816006
286.865655	7999.951347	10.306983	-0.058698	4.816003
287.041717	7999.976999	10.311987	-0.058731	4.816010
286.985852	7999.955687	10.316992	-0.058721	4.816004
286.779371	7999.860039	10.321997	-0.058682	4.815977
286.901183	7999.913555	10.327002	-0.058705	4.815992
286.775945	7999.914490	10.332007	-0.058682	4.815993
286.836244	7999.982917	10.337011	-0.058693	4.816013
286.898762	7999.971239	10.342016	-0.058705	4.816009
286.732601	7999.897696	10.347021	-0.058674	4.815988
286.814303	7999.988952	10.352026	-0.058689	4.816015
286.909001	7999.899852	10.357031	-0.058707	4.815988
286.914930	7999.955535	10.362035	-0.058708	4.816004
286.941169	7999.994490	10.367040	-0.058713	4.816015
286.826975	7999.916549	10.372045	-0.058692	4.815993
287.115507	7999.994472	10.377050	-0.058746	4.816015
286.970558	7999.953372	10.382055	-0.058719	4.816003
287.099746	7999.912987	10.387059	-0.058743	4.815991
286.880336	8000.008382	10.392064	-0.058702	4.816020
286.901586	7999.923288	10.397069	-0.058706	4.815995
286.992924	7999.978388	10.402074	-0.058723	4.816010
286.989232	7999.946271	10.407079	-0.058723	4.816001
286.921096	7999.965342	10.412083	-0.058710	4.816007
286.978673	7999.995250	10.417088	-0.058721	4.816015
286.973454	7999.957761	10.422093	-0.058720	4.816005
287.027473	7999.979055	10.427098	-0.058730	4.816010
286.944015	7999.959378	10.432103	-0.058715	4.816005
286.856980	7999.966351	10.437107	-0.058698	4.816008
287.063216	7999.941259	10.442112	-0.058737	4.815999
286.918414	7999.955730	10.447117	-0.058710	4.816004
287.050540	8000.004092	10.452122	-0.058735	4.816018
287.149134	7999.984522	10.457127	-0.058753	4.816011
287.038208	7999.968619	10.462131	-0.058733	4.816007
287.102039	8000.038179	10.467136	-0.058745	4.816027
287.044261	7999.919589	10.472141	-0.058734	4.815993
286.884321	8000.014998	10.477146	-0.058704	4.816022
286.678330	7999.981336	10.482151	-0.058666	4.816013
286.916841	7999.949352	10.487155	-0.058710	4.816002
286.954805	7999.961805	10.492160	-0.058718	4.816006
286.802035	7999.932318	10.497165	-0.058689	4.815998
286.973400	7999.982462	10.502170	-0.058721	4.816012
287.011551	7999.934008	10.507175	-0.058728	4.815997
287.084978	7999.941764	10.512179	-0.058742	4.815999
286.982374	8000.002952	10.517184	-0.058723	4.816018
287.064812	7999.883708	10.522189	-0.058738	4.815982
287.214513	7999.978339	10.527194	-0.058766	4.816009
287.273460	7999.953773	10.532199	-0.058777	4.816002
287.237872	7999.947790	10.537203	-0.058771	4.816000
287.162879	7999.979560	10.542208	-0.058757	4.816010
287.097512	7999.955938	10.547213	-0.058745	4.816003
287.025275	7999.994169	10.552218	-0.058732	4.816015
287.030399	7999.972898	10.557223	-0.058733	4.816009
287.132676	7999.949121	10.562227	-0.058752	4.816001
287.009998	7999.959719	10.567232	-0.058729	4.816005
287.004008	7999.917943	10.572237	-0.058728	4.815993
287.199021	8000.008056	10.577242	-0.058764	4.816018
287.177627	7999.980959	10.582247	-0.058760	4.816010
287.125239	7999.984288	10.587251	-0.058751	4.816011
287.171971	8000.021479	10.592256	-0.058760	4.816022
286.935884	7999.941320	10.597261	-0.058716	4.816000
287.159770	8000.015929	10.602266	-0.058757	4.816020
287.190039	7999.906421	10.607271	-0.058763	4.815988
287.089535	7999.861857	10.612275	-0.058744	4.815976
287.125172	7999.977922	10.617280	-0.058751	4.816010
286.916397	7999.916426	10.622285	-0.058712	4.815993
287.137221	7999.967470	10.627290	-0.058754	4.816006
287.019169	7999.914037	10.632295	-0.058732	4.815991
287.023781	7999.964353	10.637299	-0.058733	4.816006
286.908988	7999.990055	10.642304	-0.058711	4.816014
286.824973	7999.882744	10.647309	-0.058696	4.815983
287.052590	7999.924293	10.652314	-0.058738	4.815994
287.082429	7999.922707	10.657319	-0.058744	4.815994
287.168704	7999.987332	10.662323	-0.058760	4.816012
287.053252	7999.999131	10.667328	-0.058739	4.816016
287.187156	7999.913950	10.672333	-0.058764	4.815990
287.284433	7999.978776	10.677338	-0.058782	4.816009
287.094643	7999.979604	10.682343	-0.058747	4.816010
287.214060	7999.961481	10.687347	-0.058769	4.816004
287.314514	8000.016748	10.692352	-0.058788	4.816020
287.251082	7999.949347	10.697357	-0.058776	4.816000
287.069253	7999.981310	10.702362	-0.058742	4.816011
287.170186	7999.944685	10.707367	-0.058761	4.816000
287.075471	7999.937626	10.712371	-0.058743	4.815998
287.128248	8000.021945	10.717376	-0.058753	4.816022
286.951410	7999.967442	10.722381	-0.058721	4.816007
287.283439	7999.983109	10.727386	-0.058782	4.816010
287.206632	7999.957141	10.732391	-0.058768	4.816003
287.255879	7999.912095	10.737395	-0.058777	4.815990
287.266565	7999.948630	10.742400	-0.058780	4.816000
287.110438	7999.912670	10.747405	-0.058750	4.815990
287.187038	7999.971776	10.752410	-0.058765	4.816007
287.312795	7999.953769	10.757415	-0.058788	4.816001
287.450254	7999.990474	10.762419	-0.058814	4.816011
287.354686	8000.002634	10.767424	-0.058796	4.816015
287.295067	7999.908588	10.772429	-0.058785	4.815988
287.481450	7999.956869	10.777434	-0.058820	4.816001
287.404807	7999.906326	10.782439	-0.058806	4.815987
287.191639	7999.962297	10.787443	-0.058766	4.816005
287.219121	8000.005549	10.792448	-0.058772	4.816017
287.200545	7999.974229	10.797453	-0.058768	4.816008
287.154324	8000.004385	10.802458	-0.058760	4.816017
287.249397	7999.950555	10.807463	-0.058777	4.816001
287.298606	7999.953596	10.812467	-0.058787	4.816001
287.411736	7999.927879	10.817472	-0.058808	4.815993
287.333488	7999.894404	10.822477	-0.058793	4.815984
287.223318	8000.014228	10.827482	-0.058773	4.816020
287.194723	7999.911129	10.832487	-0.058768	4.815990
287.250516	7999.859791	10.837491	-0.058778	4.815974
287.225484	7999.943763	10.842496	-0.058773	4.815999
287.276045	7999.964994	10.847501	-0.058783	4.816005
287.516513	8000.002505	10.852506	-0.058828	4.816015
287.363002	7999.930259	10.857511	-0.058799	4.815994
287.248890	7999.888652	10.862515	-0.058778	4.815983
287.361130	7999.952682	10.867520	-0.058799	4.816001
287.408857	7999.892647	10.872525	-0.058808	4.815983
287.406404	7999.978099	10.877530	-0.058808	4.816008
287.377200	7999.944448	10.882535	-0.058802	4.815998
287.201260	7999.865384	10.887539	-0.058770	4.815976
287.367285	7999.929323	10.892544	-0.058801	4.815994
287.387877	7999.875206	10.897549	-0.058805	4.815978
287.408102	7999.933287	10.902554	-0.058808	4.815995
287.471080	7999.939784	10.907559	-0.058820	4.815996
287.335394	7999.887098	10.912563	-0.058795	4.815982
287.304865	7999.939980	10.917568	-0.058789	4.815997
287.354812	7999.956926	10.922573	-0.058799	4.816002
287.487413	7999.974308	10.927578	-0.058824	4.816006
287.272639	7999.972544	10.932583	-0.058784	4.816007
287.313646	7999.961543	10.937587	-0.058791	4.816004
287.317071	8000.058857	10.942592	-0.058792	4.816032
287.420579	7999.975260	10.947597	-0.058811	4.816007
287.604796	8000.051286	10.952602	-0.058846	4.816028
287.376066	8000.024690	10.957607	-0.058803	4.816022
287.447147	8000.014237	10.962611	-0.058817	4.816018
287.298793	8000.002995	10.967616	-0.058789	4.816016
287.338474	7999.899001	10.972621	-0.058797	4.815985
287.417990	7999.963504	10.977626	-0.058811	4.816004
287.448765	7999.986513	10.982631	-0.058817	4.816010
287.346872	7999.979323	10.987635	-0.058798	4.816009
287.117454	8000.022175	10.992640	-0.058756	4.816022
287.311464	7999.934881	10.997645	-0.058792	4.815996
287.419190	8000.038368	11.002650	-0.058812	4.816025
287.476918	7999.980652	11.007655	-0.058823	4.816008
287.382996	7999.949030	11.012659	-0.058805	4.816000
287.357759	7999.949647	11.017664	-0.058801	4.816000
287.215958	7999.870134	11.022669	-0.058774	4.815977
287.397932	7999.950393	11.027674	-0.058808	4.816000
287.407207	7999.940952	11.032679	-0.058810	4.815997
287.467674	7999.886493	11.037683	-0.058822	4.815981
287.357829	7999.988157	11.042688	-0.058801	4.816011
287.402155	8000.001794	11.047693	-0.058810	4.816015
287.394878	8000.050826	11.052698	-0.058808	4.816029
287.205930	8000.013199	11.057703	-0.058773	4.816019
287.226091	8000.007162	11.062707	-0.058777	4.816017
287.251088	7999.989459	11.067712	-0.058782	4.816012
287.254338	7999.942507	11.072717	-0.058782	4.815998
287.488791	7999.916860	11.077722	-0.058826	4.815990
287.540280	7999.897501	11.082727	-0.058836	4.815984
287.448455	7999.933239	11.087731	-0.058819	4.815995
287.415396	8000.012791	11.092736	-0.058813	4.816018
287.397696	7999.970801	11.097741	-0.058810	4.816006
287.476384	7999.912399	11.102746	-0.058824	4.815988
287.349115	7999.887649	11.107751	-0.058801	4.815982
287.305319	7999.913575	11.112755	-0.058793	4.815990
287.274075	7999.991023	11.117760	-0.058787	4.816012
287.323558	7999.960942	11.122765	-0.058796	4.816003
287.427422	8000.007721	11.127770	-0.058816	4.816016
287.684948	7999.999593	11.132775	-0.058864	4.816013
287.682045	7999.981381	11.137779	-0.058863	4.816007
287.675130	7999.971646	11.142784	-0.058862	4.816005
287.572744	7999.918496	11.147789	-0.058843	4.815990
287.532971	8000.022505	11.152794	-0.058836	4.816020
287.598138	7999.957444	11.157799	-0.058848	4.816001
287.342183	7999.910049	11.162803	-0.058800	4.815988
287.517994	7999.999814	11.167808	-0.058833	4.816014
287.514201	7999.951665	11.172813	-0.058832	4.816000
287.819883	7999.979678	11.177818	-0.058889	4.816006
287.666346	7999.884990	11.182823	-0.058861	4.815979
287.606031	7999.892449	11.187827	-0.058850	4.815982
287.498649	7999.934315	11.192832	-0.058830	4.815995
287.526145	7999.973294	11.197837	-0.058835	4.816006
287.682024	7999.934462	11.202842	-0.058864	4.815994
287.530942	7999.961642	11.207847	-0.058836	4.816002
287.469609	7999.855809	11.212851	-0.058825	4.815972
287.910975	7999.927967	11.217856	-0.058907	4.815990
287.750619	7999.895134	11.222861	-0.058877	4.815982
287.866365	7999.937856	11.227866	-0.058899	4.815994
287.693442	7999.932579	11.232871	-0.058867	4.815993
287.720269	7999.915978	11.237875	-0.058872	4.815988
287.730603	7999.993114	11.242880	-0.058874	4.816010
287.655244	7999.972515	11.247885	-0.058860	4.816005
287.911071	8000.000689	11.252890	-0.058908	4.816012
287.669872	7999.981346	11.257895	-0.058863	4.816007
287.720949	7999.974803	11.262899	-0.058872	4.816005
287.989799	7999.987185	11.267904	-0.058923	4.816007
287.796843	7999.994366	11.272909	-0.058887	4.816010
287.897960	7999.972705	11.277914	-0.058906	4.816004
287.623465	8000.005118	11.282919	-0.058855	4.816015
287.824840	7999.924370	11.287923	-0.058892	4.815990
287.723659	8000.028330	11.292928	-0.058873	4.816021
287.759714	7999.964876	11.297933	-0.058880	4.816002
287.824111	8000.037654	11.302938	-0.058892	4.816023
287.753501	7999.955161	11.307943	-0.058879	4.815999
287.748192	7999.958278	11.312947	-0.058878	4.816000
287.993645	8000.046107	11.317952	-0.058924	4.816025
287.771273	7999.969400	11.322957	-0.058883	4.816003
287.701622	8000.017296	11.327962	-0.058870	4.816018
287.737568	7999.969870	11.332967	-0.058877	4.816004
287.818791	8000.018376	11.337971	-0.058892	4.816017
287.714933	8000.003670	11.342976	-0.058873	4.816014
287.625439	7999.979608	11.347981	-0.058856	4.816007
287.788728	8000.001823	11.352986	-0.058886	4.816013
287.618002	8000.020095	11.357991	-0.058855	4.816019
287.748930	7999.976535	11.362995	-0.058879	4.816005
287.712335	8000.011142	11.368000	-0.058872	4.816016
287.717478	8000.006968	11.373005	-0.058873	4.816015
287.667545	8000.019959	11.378010	-0.058864	4.816019
287.637604	8000.009805	11.383015	-0.058859	4.816016
287.898015	7999.963259	11.388019	-0.058907	4.816001
287.951536	8000.036907	11.393024	-0.058917	4.816022
287.801232	7999.983953	11.398029	-0.058889	4.816007
287.829503	7999.973790	11.403034	-0.058895	4.816004
287.755877	8000.004516	11.408039	-0.058881	4.816014
287.681072	7999.990338	11.413043	-0.058867	4.816010
287.834454	8000.005962	11.418048	-0.058896	4.816014
287.857011	7999.929439	11.423053	-0.058900	4.815991
287.923960	7999.924254	11.428058	-0.058913	4.815989
287.772948	7999.953571	11.433063	-0.058885	4.815999
287.799521	7999.957269	11.438067	-0.058890	4.816000
287.639726	8000.018485	11.443072	-0.058860	4.816018
287.604279	7999.956936	11.448077	-0.058854	4.816000
287.786422	8000.011553	11.453082	-0.058888	4.816015
287.605251	7999.990097	11.458087	-0.058854	4.816010
287.630985	7999.978818	11.463091	-0.058859	4.816007
287.569791	8000.042898	11.468096	-0.058848	4.816026
287.775017	7999.947259	11.473101	-0.058886	4.815997
287.718108	7999.984701	11.478106	-0.058875	4.816008
288.024999	7999.981747	11.483111	-0.058932	4.816005
288.045789	7999.923358	11.488115	-0.058936	4.815988
287.900856	7999.982708	11.493120	-0.058910	4.816006
287.892452	7999.919514	11.498125	-0.058908	4.815988
287.942451	7999.928981	11.503130	-0.058917	4.815990
287.907203	7999.990327	11.508135	-0.058911	4.816009
287.866607	7999.895557	11.513139	-0.058903	4.815981
288.020177	7999.984919	11.518144	-0.058932	4.816006
288.074518	7999.921798	11.523149	-0.058942	4.815988
288.136612	7999.918662	11.528154	-0.058954	4.815986
288.023381	7999.932638	11.533159	-0.058933	4.815991
287.864462	7999.915861	11.538163	-0.058903	4.815987
287.977891	7999.999149	11.543168	-0.058925	4.816011
287.815922	7999.978041	11.548173	-0.058895	4.816005
287.924175	7999.945824	11.553178	-0.058915	4.815995
287.820079	7999.999505	11.558183	-0.058896	4.816012
287.708673	7999.963289	11.563187	-0.058875	4.816002
287.965693	8000.009652	11.568192	-0.058923	4.816014
287.882756	7999.893807	11.573197	-0.058907	4.815981
288.043328	7999.981159	11.578202	-0.058937	4.816005
287.881205	7999.966460	11.583207	-0.058907	4.816002
287.892408	7999.937819	11.588211	-0.058909	4.815993
288.026813	7999.978744	11.593216	-0.058935	4.816005
287.927521	7999.991905	11.598221	-0.058916	4.816009
287.925090	8000.033545	11.603226	-0.058916	4.816021
287.812195	8000.026155	11.608231	-0.058895	4.816020
287.726260	7999.943383	11.613235	-0.058879	4.815996
287.960856	7999.981857	11.618240	-0.058923	4.816006
287.985449	7999.997273	11.623245	-0.058927	4.816010
288.053775	7999.972877	11.628250	-0.058940	4.816003
287.835209	7999.886623	11.633255	-0.058899	4.815979
287.906271	7999.859071	11.638259	-0.058913	4.815970
288.001901	7999.960201	11.643264	-0.058931	4.815999
287.961608	7999.898564	11.648269	-0.058923	4.815981
287.825410	7999.932426	11.653274	-0.058898	4.815992
287.746312	7999.924582	11.658279	-0.058883	4.815990
287.860557	7999.879650	11.663283	-0.058905	4.815976
287.864869	7999.948128	11.668288	-0.058906	4.815996
287.821272	7999.894980	11.673293	-0.058897	4.815981
287.886308	7999.934642	11.678298	-0.058910	4.815992
287.808214	8000.006963	11.683303	-0.058895	4.816014
287.959793	7999.931720	11.688307	-0.058924	4.815991
287.858230	8000.010026	11.693312	-0.058905	4.816015
287.777410	7999.940171	11.698317	-0.058890	4.815995
287.978389	7999.927807	11.703322	-0.058927	4.815990
287.858832	7999.937394	11.708327	-0.058905	4.815993
287.868391	7999.899105	11.713331	-0.058907	4.815982
287.981458	7999.981318	11.718336	-0.058928	4.816005
287.905103	7999.953220	11.723341	-0.058914	4.815998
288.012709	7999.948775	11.728346	-0.058934	4.815996
287.885832	7999.961434	11.733351	-0.058911	4.816000
287.968375	7999.887072	11.738355	-0.058926	4.815978
288.127649	7999.978675	11.743360	-0.058956	4.816004
287.995664	7999.961319	11.748365	-0.058931	4.816000
287.989333	7999.941976	11.753370	-0.058930	4.815994
287.952120	7999.958405	11.758375	-0.058923	4.815999
288.055834	7999.950683	11.763379	-0.058943	4.815996
288.121383	8000.008521	11.768384	-0.058955	4.816013
287.953250	7999.966997	11.773389	-0.058924	4.816001
287.912759	7999.954513	11.778394	-0.058916	4.815998
287.970558	7999.981220	11.783399	-0.058927	4.816005
288.144381	7999.972637	11.788403	-0.058960	4.816002
288.198063	7999.992858	11.793408	-0.058970	4.816008
287.943931	7999.948700	11.798413	-0.058922	4.815996
287.910326	7999.959851	11.803418	-0.058916	4.816000
288.027040	7999.980150	11.808423	-0.058938	4.816005
288.199824	7999.909568	11.813427	-0.058970	4.815983
288.055246	7999.994571	11.818432	-0.058943	4.816009
288.005642	7999.995813	11.823437	-0.058934	4.816010
288.011732	8000.013030	11.828442	-0.058935	4.816015
287.830946	7999.971276	11.833447	-0.058902	4.816003
287.757428	7999.881250	11.838451	-0.058888	4.815977
288.139594	7999.958743	11.843456	-0.058959	4.815998
288.158150	7999.880010	11.848461	-0.058963	4.815975
288.020851	7999.928813	11.853466	-0.058938	4.815990
287.869091	7999.947430	11.858471	-0.058909	4.815996
288.027376	7999.909712	11.863475	-0.058939	4.815984
288.067185	7999.956395	11.868480	-0.058946	4.815998
287.973908	7999.898068	11.873485	-0.058929	4.815981
287.971682	7999.940780	11.878490	-0.058929	4.815994
287.838021	7999.953315	11.883495	-0.058904	4.815998
287.978092	7999.947324	11.888499	-0.058930	4.815995
287.921052	7999.977283	11.893504	-0.058920	4.816005
287.788955	7999.924661	11.898509	-0.058895	4.815990
287.902889	7999.945978	11.903514	-0.058916	4.815995
287.954411	7999.909522	11.908519	-0.058926	4.815985
287.994284	7999.908118	11.913523	-0.058934	4.815984
288.062300	8000.032256	11.918528	-0.058946	4.816020
288.014005	7999.943757	11.923533	-0.058937	4.815994
288.186302	7999.952245	11.928538	-0.058970	4.815996
288.026227	7999.981397	11.933543	-0.058940	4.816005
287.786701	7999.925751	11.938547	-0.058895	4.815990
288.213962	7999.955977	11.943552	-0.058975	4.815997
288.237218	7999.896565	11.948557	-0.058979	4.815979
288.330319	7999.957043	11.953562	-0.058997	4.815996
288.121140	7999.973546	11.958567	-0.058958	4.816002
287.914618	7999.897128	11.963571	-0.058919	4.815981
288.087716	7999.916316	11.968576	-0.058952	4.815986
287.954567	7999.961988	11.973581	-0.058927	4.816000
288.219970	7999.956141	11.978586	-0.058977	4.815997
288.091716	7999.905726	11.983591	-0.058953	4.815983
288.015212	7999.935331	11.988595	-0.058939	4.815992
288.119154	7999.997074	11.993600	-0.058958	4.816009
288.121603	7999.939420	11.998605	-0.058959	4.815992
288.168755	7999.999061	12.003610	-0.058967	4.816010
288.052267	7999.932831	12.008615	-0.058946	4.815991
288.128998	7999.894696	12.013619	-0.058960	4.815979
288.242603	7999.950203	12.018624	-0.058981	4.815995
288.133488	7999.925783	12.023629	-0.058961	4.815988
288.366714	7999.973851	12.028634	-0.059005	4.816001
288.192863	8000.001684	12.033639	-0.058972	4.816010
288.043884	7999.974401	12.038643	-0.058945	4.816003
288.103277	8000.032128	12.043648	-0.058956	4.816020
288.197957	7999.948368	12.048653	-0.058974	4.815995
288.193385	7999.995313	12.053658	-0.058973	4.816008
288.125417	7999.996220	12.058663	-0.058960	4.816009
288.160705	7999.942370	12.063667	-0.058967	4.815993
288.288513	8000.041951	12.068672	-0.058991	4.816021
288.169446	7999.971398	12.073677	-0.058969	4.816001
288.261540	8000.027583	12.078682	-0.058986	4.816017
288.284172	7999.997012	12.083687	-0.058990	4.816008
288.288245	7999.999231	12.088691	-0.058991	4.816009
288.257910	7999.989069	12.093696	-0.058986	4.816006
288.153473	7999.990381	12.098701	-0.058966	4.816007
288.235530	7999.942726	12.103706	-0.058981	4.815993
288.254531	7999.938805	12.108711	-0.058985	4.815991
288.394494	7999.948841	12.113715	-0.059011	4.815994
288.428775	8000.010386	12.118720	-0.059018	4.816011
288.284916	7999.987470	12.123725	-0.058991	4.816005
288.399359	7999.998110	12.128730	-0.059012	4.816008
288.287762	7999.971508	12.133735	-0.058992	4.816001
288.176237	7999.909641	12.138739	-0.058971	4.815983
288.299112	8000.003789	12.143744	-0.058994	4.816010
288.110774	7999.926632	12.148749	-0.058959	4.815989
288.289781	7999.986536	12.153754	-0.058992	4.816005
288.198951	7999.962449	12.158759	-0.058976	4.815999
288.134377	7999.914261	12.163763	-0.058964	4.815985
288.286080	7999.953364	12.168768	-0.058992	4.815995
288.217412	7999.929681	12.173773	-0.058979	4.815989
288.330766	7999.937095	12.178778	-0.059000	4.815990
288.199567	7999.979597	12.183783	-0.058976	4.816004
288.186770	7999.981509	12.188787	-0.058974	4.816004
288.245541	7999.924881	12.193792	-0.058985	4.815987
288.124372	7999.923751	12.198797	-0.058962	4.815988
288.211907	7999.957411	12.203802	-0.058979	4.815997
288.192957	7999.913260	12.208807	-0.058975	4.815984
288.195956	7999.863097	12.213811	-0.058976	4.815970
288.208506	7999.936000	12.218816	-0.058978	4.815991
288.164728	7999.919181	12.223821	-0.058970	4.815986
288.246793	7999.966634	12.228826	-0.058986	4.816000
288.356139	7999.973976	12.233831	-0.059006	4.816001
288.218117	7999.944755	12.238835	-0.058980	4.815993
288.407521	7999.931113	12.243840	-0.059016	4.815988
288.449474	7999.934022	12.248845	-0.059024	4.815989
288.464613	7999.925756	12.253850	-0.059026	4.815986
288.212449	7999.992771	12.258855	-0.058980	4.816007
288.374286	7999.861077	12.263859	-0.059010	4.815968
288.565983	7999.947929	12.268864	-0.059046	4.815992
288.464068	7999.857384	12.273869	-0.059027	4.815966
288.332675	8000.007815	12.278874	-0.059002	4.816011
288.562623	8000.019490	12.283879	-0.059045	4.816013
288.414740	8000.008256	12.288883	-0.059018	4.816011
288.486962	8000.045913	12.293888	-0.059031	4.816021
288.473135	7999.960177	12.298893	-0.059029	4.815996
288.474775	7999.923881	12.303898	-0.059029	4.815986
288.552397	7999.990489	12.308903	-0.059044	4.816005
288.499470	7999.953199	12.313907	-0.059034	4.815994
288.503510	8000.002438	12.318912	-0.059035	4.816009
288.397657	7999.898998	12.323917	-0.059015	4.815979
288.376952	8000.049307	12.328922	-0.059011	4.816023
288.536069	8000.058624	12.333927	-0.059041	4.816025
288.467543	8000.024256	12.338931	-0.059028	4.816015
288.273487	8000.083780	12.343936	-0.058992	4.816034
288.392848	8000.021843	12.348941	-0.059015	4.816015
288.319457	7999.947847	12.353946	-0.059001	4.815994
288.355909	8000.003019	12.358951	-0.059008	4.816010
288.158002	7999.920344	12.363955	-0.058971	4.815986
288.227881	7999.938722	12.368960	-0.058984	4.815991
288.353065	7999.934597	12.373965	-0.059008	4.815990
288.426904	7999.959459	12.378970	-0.059021	4.815996
288.325857	7999.965108	12.383975	-0.059003	4.815999
288.214672	7999.910728	12.388979	-0.058982	4.815983
288.464305	7999.941997	12.393984	-0.059029	4.815991
288.348326	7999.917452	12.398989	-0.059007	4.815985
288.582391	7999.973016	12.403994	-0.059051	4.816000
288.373773	7999.986323	12.408999	-0.059012	4.816005
288.337589	7999.993153	12.414003	-0.059005	4.816007
288.322749	8000.009988	12.419008	-0.059003	4.816012
288.318562	7999.969312	12.424013	-0.059002	4.816000
288.261245	7999.981099	12.429018	-0.058991	4.816004
288.531704	8000.027709	12.434023	-0.059042	4.816016
288.429153	8000.006614	12.439027	-0.059023	4.816010
288.538455	8000.026778	12.444032	-0.059043	4.816015
288.440783	8000.003635	12.449037	-0.059025	4.816009
288.440691	8000.005778	12.454042	-0.059025	4.816010
288.307299	8000.023661	12.459047	-0.059001	4.816016
288.162901	7999.997530	12.464051	-0.058974	4.816009
288.332473	8000.065812	12.469056	-0.059005	4.816028
288.309788	7999.988465	12.474061	-0.059001	4.816005
288.278787	7999.951574	12.479066	-0.058995	4.815995
288.356952	7999.938044	12.484071	-0.059010	4.815990
288.321168	7999.950224	12.489075	-0.059004	4.815994
288.395856	7999.971896	12.494080	-0.059018	4.816000
288.379803	7999.938484	12.499085	-0.059015	4.815990
288.403186	7999.917544	12.504090	-0.059019	4.815984
288.460967	7999.972036	12.509095	-0.059030	4.816000
288.356095	7999.910291	12.514099	-0.059010	4.815982
288.583745	7999.927267	12.519104	-0.059053	4.815986
288.507971	7999.883149	12.524109	-0.059039	4.815974
288.359351	7999.917854	12.529114	-0.059011	4.815985
288.308287	7999.924412	12.534119	-0.059002	4.815987
288.521455	7999.872732	12.539123	-0.059042	4.815971
288.649562	7999.969112	12.544128	-0.059066	4.815998
288.287319	7999.914436	12.549133	-0.058998	4.815984
288.452625	7999.921728	12.554138	-0.059029	4.815985
288.399170	7999.930380	12.559143	-0.059019	4.815988
288.344533	7999.917638	12.564147	-0.059009	4.815985
288.543947	7999.955473	12.569152	-0.059046	4.815995
288.405218	7999.933719	12.574157	-0.059020	4.815989
288.386324	7999.918422	12.579162	-0.059017	4.815985
288.373672	7999.990867	12.584167	-0.059015	4.816006
288.319776	7999.908677	12.589171	-0.059005	4.815982
288.420470	7999.962881	12.594176	-0.059024	4.815997
288.261461	7999.919386	12.599181	-0.058994	4.815985
288.573027	7999.958194	12.604186	-0.059052	4.815995
288.553032	7999.995240	12.609191	-0.059049	4.816006
288.278178	7999.973145	12.614195	-0.058998	4.816001
288.510638	7999.993415	12.619200	-0.059041	4.816006
288.490464	7999.977026	12.624205	-0.059037	4.816001
288.463026	7999.940200	12.629210	-0.059032	4.815990
288.536909	8000.004603	12.634215	-0.059046	4.816009
288.519692	7999.944453	12.639219	-0.059043	4.815991
288.491771	8000.015552	12.644224	-0.059038	4.816012
288.395945	7999.951833	12.649229	-0.059020	4.815994
288.362134	7999.954431	12.654234	-0.059014	4.815995
288.398597	7999.991437	12.659239	-0.059021	4.816006
288.485541	7999.887232	12.664243	-0.059037	4.815975
288.406219	7999.988385	12.669248	-0.059022	4.816005
288.239748	7999.973607	12.674253	-0.058991	4.816001
288.437003	7999.924843	12.679258	-0.059028	4.815986
288.366595	7999.956696	12.684263	-0.059015	4.815996
288.564838	7999.917568	12.689267	-0.059052	4.815983
288.558054	7999.922795	12.694272	-0.059051	4.815985
288.474226	7999.874257	12.699277	-0.059035	4.815971
288.687472	7999.897383	12.704282	-0.059075	4.815977
288.592420	7999.926650	12.709287	-0.059057	4.815986
288.372860	7999.915180	12.714291	-0.059017	4.815984
288.313212	8000.031652	12.719296	-0.059006	4.816018
288.519669	7999.995879	12.724301	-0.059044	4.816006
288.432753	8000.006060	12.729306	-0.059028	4.816010
288.351167	7999.990689	12.734311	-0.059013	4.816006
288.415084	7999.901027	12.739315	-0.059025	4.815979
288.575084	7999.957380	12.744320	-0.059055	4.815995
288.410558	7999.903097	12.749325	-0.059024	4.815980
288.569521	7999.956225	12.754330	-0.059054	4.815995
288.680933	7999.987115	12.759335	-0.059075	4.816003
288.661803	7999.926930	12.764339	-0.059071	4.815985
288.619048	7999.984935	12.769344	-0.059063	4.816003
288.489357	7999.925943	12.774349	-0.059039	4.815986
288.506985	7999.925203	12.779354	-0.059043	4.815986
288.413225	7999.982279	12.784359	-0.059025	4.816003
288.447259	7999.904896	12.789363	-0.059032	4.815980
288.663185	7999.918453	12.794368	-0.059072	4.815983
288.495179	7999.937843	12.799373	-0.059041	4.815990
288.648633	7999.993008	12.804378	-0.059070	4.816005
288.604987	7999.998633	12.809383	-0.059061	4.816007
288.535163	7999.938594	12.814387	-0.059048	4.815990
288.543480	7999.970813	12.819392	-0.059050	4.815999
288.456729	7999.941456	12.824397	-0.059034	4.815991
288.638700	7999.925542	12.829402	-0.059068	4.815985
288.674707	8000.003148	12.834407	-0.059075	4.816008
288.454802	7999.925415	12.839411	-0.059034	4.815986
288.522256	8000.007868	12.844416	-0.059047	4.816010
288.303040	7999.935491	12.849421	-0.059006	4.815990
288.372615	7999.928216	12.854426	-0.059019	4.815987
288.484506	7999.964458	12.859431	-0.059040	4.815997
288.330733	7999.892204	12.864435	-0.059011	4.815977
288.390654	7999.978794	12.869440	-0.059022	4.816002
288.588466	7999.912942	12.874445	-0.059059	4.815982
288.716883	7999.950553	12.879450	-0.059083	4.815992
288.365161	7999.951637	12.884455	-0.059018	4.815994
288.388623	7999.885816	12.889459	-0.059022	4.815975
288.597442	7999.983667	12.894464	-0.059061	4.816002
288.500931	7999.950926	12.899469	-0.059043	4.815993
288.463265	7999.947042	12.904474	-0.059037	4.815992
288.476009	7999.941939	12.909479	-0.059039	4.815991
288.487163	7999.949630	12.914483	-0.059041	4.815993
288.518948	8000.028228	12.919488	-0.059047	4.816016
288.448772	7999.963908	12.924493	-0.059034	4.815997
288.498274	7999.935963	12.929498	-0.059043	4.815989
288.461716	7999.982326	12.934503	-0.059037	4.816003
288.521266	7999.920368	12.939507	-0.059048	4.815984
288.542625	8000.013737	12.944512	-0.059052	4.816011
288.701752	7999.945043	12.949517	-0.059082	4.815990
288.375991	7999.961560	12.954522	-0.059021	4.815997
288.620991	7999.916871	12.959527	-0.059067	4.815983
288.659407	7999.882313	12.964531	-0.059074	4.815972
288.647044	7999.932322	12.969536	-0.059072	4.815987
288.499771	7999.941404	12.974541	-0.059044	4.815990
288.554194	7999.952020	12.979546	-0.059055	4.815993
288.436483	7999.928512	12.984551	-0.059033	4.815987
288.269993	7999.859233	12.989555	-0.059002	4.815968
288.665665	7999.910258	12.994560	-0.059076	4.815981
288.832030	7999.869481	12.999565	-0.059107	4.815968
288.589413	7999.888581	13.004570	-0.059062	4.815975
288.599709	7999.909081	13.009575	-0.059064	4.815981
288.486200	7999.889924	13.014579	-0.059043	4.815976
288.701430	7999.922704	13.019584	-0.059083	4.815984
288.607071	7999.859012	13.024589	-0.059065	4.815966
288.639769	7999.893812	13.029594	-0.059071	4.815976
288.529007	7999.890734	13.034599	-0.059051	4.815976
288.684721	7999.883959	13.039603	-0.059080	4.815973
288.892829	7999.915541	13.044608	-0.059119	4.815981
288.820456	7999.880034	13.049613	-0.059105	4.815971
288.632358	7999.884098	13.054618	-0.059070	4.815973
288.507450	7999.978009	13.059623	-0.059047	4.816001
288.730172	7999.883757	13.064627	-0.059089	4.815972
288.726378	7999.917892	13.069632	-0.059088	4.815982
288.590157	7999.868399	13.074637	-0.059063	4.815969
288.723810	7999.884733	13.079642	-0.059088	4.815973
288.814092	7999.904551	13.084647	-0.059105	4.815978
288.540346	7999.887820	13.089651	-0.059054	4.815975
288.737612	7999.903174	13.094656	-0.059091	4.815978
288.790923	7999.834691	13.099661	-0.059101	4.815958
288.916586	7999.873321	13.104666	-0.059124	4.815968
288.697639	7999.888577	13.109671	-0.059083	4.815974
288.624724	7999.873365	13.114675	-0.059070	4.815970
288.708409	7999.929397	13.119680	-0.059086	4.815986
288.686839	7999.825354	13.124685	-0.059082	4.815956
288.655576	7999.885705	13.129690	-0.059076	4.815973
288.576303	7999.943045	13.134695	-0.059061	4.815990
288.534476	7999.870692	13.139699	-0.059053	4.815970
288.688367	7999.905561	13.144704	-0.059082	4.815979
288.698207	7999.899336	13.149709	-0.059084	4.815977
288.766084	7999.883481	13.154714	-0.059097	4.815972
288.727303	7999.913774	13.159719	-0.059090	4.815981
288.848445	7999.889271	13.164723	-0.059112	4.815973
288.818889	7999.933624	13.169728	-0.059107	4.815986
288.575763	7999.843713	13.174733	-0.059062	4.815961
288.555559	7999.940600	13.179738	-0.059058	4.815990
288.791226	7999.890397	13.184743	-0.059102	4.815974
288.554645	7999.868999	13.189747	-0.059058	4.815969
288.829124	7999.942398	13.194752	-0.059109	4.815989
288.848043	7999.924583	13.199757	-0.059113	4.815984
288.797855	7999.935432	13.204762	-0.059104	4.815987
288.771813	7999.956339	13.209767	-0.059099	4.815993
288.883210	7999.856854	13.214771	-0.059120	4.815964
288.881108	7999.879265	13.219776	-0.059119	4.815970
288.706759	7999.869686	13.224781	-0.059087	4.815968
288.733590	7999.859496	13.229786	-0.059092	4.815965
288.626825	7999.889619	13.234791	-0.059072	4.815975
288.597478	7999.836729	13.239795	-0.059067	4.815959
288.796380	7999.886310	13.244800	-0.059104	4.815973
288.732704	7999.873403	13.249805	-0.059092	4.815969
288.645497	7999.839764	13.254810	-0.059076	4.815960
288.536183	7999.909380	13.259815	-0.059056	4.815981
288.552598	7999.873353	13.264819	-0.059059	4.815970
288.578673	7999.906963	13.269824	-0.059064	4.815980
288.668110	7999.906462	13.274829	-0.059081	4.815979
288.621844	7999.904559	13.279834	-0.059072	4.815979
288.531635	7999.927503	13.284839	-0.059055	4.815986
288.607801	7999.878671	13.289843	-0.059070	4.815971
288.537641	7999.982129	13.294848	-0.059057	4.816002
288.697400	7999.889936	13.299853	-0.059086	4.815974
288.805152	7999.888700	13.304858	-0.059107	4.815973
288.666229	7999.885109	13.309863	-0.059081	4.815973
288.698242	7999.846160	13.314867	-0.059087	4.815961
288.911215	7999.909890	13.319872	-0.059127	4.815979
288.654729	7999.924463	13.324877	-0.059079	4.815985
288.586843	7999.886901	13.329882	-0.059066	4.815974
288.705467	7999.855940	13.334887	-0.059088	4.815964
288.761046	7999.820626	13.339891	-0.059099	4.815954
288.837515	7999.909655	13.344896	-0.059113	4.815979
288.797398	7999.887560	13.349901	-0.059106	4.815973
288.666031	7999.880901	13.354906	-0.059081	4.815972
288.587813	7999.883759	13.359911	-0.059067	4.815973
288.734949	7999.850112	13.364915	-0.059094	4.815962
288.726208	7999.913010	13.369920	-0.059093	4.815981
288.602924	7999.879783	13.374925	-0.059070	4.815972
288.678219	7999.900397	13.379930	-0.059084	4.815977
288.771794	7999.870049	13.384935	-0.059102	4.815968
288.811061	7999.832301	13.389939	-0.059109	4.815957
288.841076	7999.870258	13.394944	-0.059115	4.815968
288.694013	7999.871862	13.399949	-0.059087	4.815969
288.858380	7999.885549	13.404954	-0.059118	4.815972
288.758141	7999.922203	13.409959	-0.059099	4.815983
288.690892	7999.837632	13.414963	-0.059087	4.815959
288.892181	7999.871227	13.419968	-0.059125	4.815968
288.934913	7999.838885	13.424973	-0.059133	4.815958
288.935584	7999.892337	13.429978	-0.059133	4.815974
288.931360	7999.914709	13.434983	-0.059132	4.815980
288.828719	7999.874377	13.439987	-0.059113	4.815969
288.653996	7999.934253	13.444992	-0.059081	4.815987
288.934695	7999.922274	13.449997	-0.059133	4.815982
288.851720	7999.936801	13.455002	-0.059118	4.815987
288.811667	7999.971344	13.460007	-0.059110	4.815997
288.948830	7999.905456	13.465011	-0.059136	4.815977
288.926362	8000.020470	13.470016	-0.059132	4.816011
288.886032	7999.984477	13.475021	-0.059124	4.816001
288.946742	7999.912922	13.480026	-0.059136	4.815980
288.919618	7999.988310	13.485031	-0.059131	4.816002
288.743671	7999.888935	13.490035	-0.059098	4.815974
288.770004	7999.908658	13.495040	-0.059103	4.815979
288.634561	7999.831395	13.500045	-0.059078	4.815957
288.771983	7999.848866	13.505050	-0.059103	4.815962
288.703453	7999.882891	13.510055	-0.059091	4.815972
288.577789	7999.848551	13.515059	-0.059067	4.815963
288.829642	7999.926881	13.520064	-0.059114	4.815984
288.766748	7999.915057	13.525069	-0.059103	4.815981
288.856372	7999.898530	13.530074	-0.059120	4.815976
288.684561	7999.979832	13.535079	-0.059088	4.816000
288.682642	7999.890039	13.540083	-0.059087	4.815974
288.539943	7999.939812	13.545088	-0.059061	4.815990
288.726850	7999.920781	13.550093	-0.059096	4.815983
288.708749	7999.888400	13.555098	-0.059093	4.815974
288.724633	7999.936786	13.560103	-0.059096	4.815988
288.731618	7999.900587	13.565107	-0.059097	4.815977
288.968280	7999.910248	13.570112	-0.059141	4.815979
288.805491	7999.831417	13.575117	-0.059111	4.815956
288.795025	7999.870774	13.580122	-0.059109	4.815968
288.856076	7999.963798	13.585127	-0.059120	4.815995
288.929783	7999.891411	13.590131	-0.059134	4.815973
288.785269	7999.883444	13.595136	-0.059107	4.815972
288.721616	7999.909008	13.600141	-0.059096	4.815980
288.747743	7999.927659	13.605146	-0.059101	4.815985
288.838246	7999.959237	13.610151	-0.059118	4.815994
288.808990	7999.940545	13.615155	-0.059112	4.815988
288.927097	7999.997205	13.620160	-0.059134	4.816004
288.653960	7999.940943	13.625165	-0.059083	4.815989
288.726747	7999.929453	13.630170	-0.059097	4.815985
288.810742	7999.949157	13.635175	-0.059113	4.815991
288.801451	7999.877396	13.640179	-0.059111	4.815970
288.882135	7999.937649	13.645184	-0.059126	4.815987
288.772518	7999.891846	13.650189	-0.059106	4.815974
288.828449	7999.883254	13.655194	-0.059116	4.815971
288.864373	7999.932005	13.660199	-0.059123	4.815985
288.892049	7999.882290	13.665203	-0.059128	4.815971
288.871715	7999.896889	13.670208	-0.059125	4.815975
288.882363	7999.899228	13.675213	-0.059127	4.815976
288.720080	7999.893075	13.680218	-0.059097	4.815975
288.863714	7999.924551	13.685223	-0.059123	4.815983
288.906112	7999.875105	13.690227	-0.059131	4.815969
288.891818	7999.915461	13.695232	-0.059129	4.815981
288.531338	7999.918522	13.700237	-0.059062	4.815983
288.790319	7999.876225	13.705242	-0.059110	4.815970
288.738549	7999.935135	13.710247	-0.059101	4.815987
288.493787	7999.840920	13.715251	-0.059055	4.815961
288.965111	7999.886912	13.720256	-0.059143	4.815972
288.947628	7999.902631	13.725261	-0.059140	4.815976
288.643228	7999.893890	13.730266	-0.059083	4.815976
288.659116	7999.933727	13.735271	-0.059086	4.815987
288.673749	7999.845304	13.740275	-0.059089	4.815961
288.599757	7999.913426	13.745280	-0.059075	4.815981
288.629390	7999.828482	13.750285	-0.059081	4.815956
288.786979	7999.824947	13.755290	-0.059110	4.815955
288.828270	7999.867384	13.760295	-0.059118	4.815967
288.691113	7999.838178	13.765299	-0.059093	4.815959
288.835312	7999.895312	13.770304	-0.059119	4.815975
288.741481	7999.853003	13.775309	-0.059102	4.815963
288.899998	7999.868721	13.780314	-0.059132	4.815967
288.754784	7999.963331	13.785319	-0.059105	4.815995
288.886988	7999.892010	13.790323	-0.059129	4.815974
288.918519	7999.946024	13.795328	-0.059135	4.815989
288.933060	7999.891796	13.800333	-0.059138	4.815973
288.874568	7999.902493	13.805338	-0.059127	4.815977
288.897817	7999.964906	13.810343	-0.059132	4.815995
288.724153	7999.886946	13.815347	-0.059099	4.815973
289.062708	7999.931590	13.820352	-0.059163	4.815984
288.820929	7999.920783	13.825357	-0.059118	4.815982
288.942741	7999.899499	13.830362	-0.059140	4.815976
289.123215	7999.974393	13.835367	-0.059174	4.815996
288.809901	7999.855418	13.840371	-0.059116	4.815963
289.049190	7999.930314	13.845376	-0.059161	4.815984
288.987951	7999.939893	13.850381	-0.059149	4.815987
288.782121	7999.912642	13.855386	-0.059111	4.815980
289.051402	7999.959232	13.860391	-0.059161	4.815992
288.845875	7999.860386	13.865395	-0.059123	4.815965
288.785875	7999.935176	13.870400	-0.059112	4.815987
288.789596	7999.918153	13.875405	-0.059113	4.815982
288.882528	7999.899548	13.880410	-0.059130	4.815976
288.822258	7999.931587	13.885415	-0.059119	4.815985
288.684069	7999.890607	13.890419	-0.059093	4.815974
288.972151	7999.909753	13.895424	-0.059147	4.815978
288.932966	7999.913322	13.900429	-0.059140	4.815980
289.066937	7999.891190	13.905434	-0.059165	4.815972
289.249918	7999.908423	13.910439	-0.059199	4.815976
288.920036	7999.867158	13.915443	-0.059138	4.815966
289.050175	7999.884496	13.920448	-0.059162	4.815971
289.102326	7999.870493	13.925453	-0.059172	4.815966
289.079892	7999.886122	13.930458	-0.059168	4.815971
289.072240	7999.937285	13.935463	-0.059166	4.815986
289.021797	7999.848745	13.940467	-0.059157	4.815960
289.269054	7999.803029	13.945472	-0.059203	4.815946
289.144902	7999.815737	13.950477	-0.059180	4.815950
289.110391	7999.898471	13.955482	-0.059174	4.815974
289.091336	7999.884239	13.960487	-0.059170	4.815970
289.002100	7999.876210	13.965491	-0.059154	4.815968
288.981803	7999.939967	13.970496	-0.059150	4.815987
289.025890	7999.894826	13.975501	-0.059158	4.815974
289.017452	7999.901092	13.980506	-0.059157	4.815976
289.032449	7999.948393	13.985511	-0.059160	4.815989
289.079230	7999.874447	13.990515	-0.059168	4.815967
289.122811	7999.966085	13.995520	-0.059177	4.815994
289.021252	7999.961037	14.000525	-0.059158	4.815993
289.090408	7999.908871	14.005530	-0.059171	4.815977
289.295818	7999.955366	14.010535	-0.059209	4.815990
289.139900	7999.919406	14.015539	-0.059180	4.815980
289.176536	7999.967102	14.020544	-0.059187	4.815994
289.094179	7999.954923	14.025549	-0.059172	4.815991
289.183776	7999.908473	14.030554	-0.059188	4.815977
289.062633	7999.959707	14.035559	-0.059166	4.815992
288.863558	7999.851362	14.040563	-0.059129	4.815962
289.295887	7999.900920	14.045568	-0.059210	4.815974
289.160152	7999.877083	14.050573	-0.059184	4.815968
289.148686	7999.880087	14.055578	-0.059182	4.815969
289.125089	8000.003630	14.060583	-0.059178	4.816005
289.281087	7999.953046	14.065587	-0.059207	4.815989
289.260659	7999.956956	14.070592	-0.059203	4.815990
289.085951	7999.907830	14.075597	-0.059171	4.815977
289.207257	7999.911115	14.080602	-0.059194	4.815977
289.204336	7999.958091	14.085607	-0.059193	4.815991
289.081366	7999.902426	14.090611	-0.059170	4.815976
289.284242	7999.916815	14.095616	-0.059208	4.815979
289.320234	7999.908929	14.100621	-0.059215	4.815976
289.156648	7999.908095	14.105626	-0.059185	4.815977
289.270055	7999.967876	14.110631	-0.059206	4.815994
289.253709	7999.913084	14.115635	-0.059203	4.815978
289.246237	7999.942878	14.120640	-0.059202	4.815986
289.280560	7999.902902	14.125645	-0.059208	4.815975
289.349148	7999.893472	14.130650	-0.059221	4.815971
289.154048	7999.981832	14.135655	-0.059185	4.815998
289.037896	7999.894231	14.140659	-0.059163	4.815973
289.094932	7999.951917	14.145664	-0.059174	4.815990
289.266113	7999.972141	14.150669	-0.059206	4.815995
289.096547	7999.920970	14.155674	-0.059174	4.815981
289.381987	7999.983885	14.160679	-0.059228	4.815998
289.201718	7999.891910	14.165683	-0.059194	4.815972
289.279067	7999.909357	14.170688	-0.059208	4.815976
289.274869	7999.916768	14.175693	-0.059208	4.815979
289.321448	7999.893045	14.180698	-0.059216	4.815971
289.233369	7999.958775	14.185703	-0.059200	4.815991
289.155252	7999.895377	14.190707	-0.059186	4.815973
289.422407	7999.942997	14.195712	-0.059236	4.815985
289.447871	7999.956293	14.200717	-0.059240	4.815989
289.239074	7999.908682	14.205722	-0.059202	4.815976
289.196689	7999.943184	14.210727	-0.059194	4.815987
289.203613	7999.849276	14.215731	-0.059195	4.815959
289.174102	7999.940651	14.220736	-0.059190	4.815986
289.159205	7999.921151	14.225741	-0.059187	4.815981
289.215743	7999.918983	14.230746	-0.059198	4.815980
289.084619	7999.970035	14.235751	-0.059173	4.815995
289.188654	7999.885377	14.240755	-0.059193	4.815970
289.314051	7999.940033	14.245760	-0.059216	4.815985
289.226709	7999.982265	14.250765	-0.059200	4.815998
289.108346	7999.897830	14.255770	-0.059178	4.815974
289.227210	7999.963053	14.260775	-0.059200	4.815992
289.219651	7999.927658	14.265779	-0.059199	4.815982
289.272413	7999.941450	14.270784	-0.059209	4.815986
289.046434	7999.959784	14.275789	-0.059167	4.815992
289.211398	7999.465875	14.280794	-0.059197	4.815847

289.247565	7996.062231	14.285799	-0.059202	4.814853
289.106290	7990.629862	14.290803	-0.059172	4.813266
289.123048	7983.976471	14.295808	-0.059171	4.811320
289.118721	7976.632808	14.300813	-0.059165	4.809172
288.949513	7969.023959	14.305818	-0.059129	4.806947
289.047011	7961.203684	14.310823	-0.059142	4.804657
288.954202	7953.361482	14.315827	-0.059120	4.802360
289.132189	7945.396637	14.320832	-0.059148	4.800025
289.028343	7937.482006	14.325837	-0.059124	4.797705
288.942645	7929.389595	14.330842	-0.059102	4.795332
289.015115	7921.414418	14.335847	-0.059111	4.792991
288.908719	7913.299920	14.340851	-0.059086	4.790609
288.750882	7905.413936	14.345856	-0.059051	4.788293
288.585225	7897.389409	14.350861	-0.059015	4.785935
288.489087	7889.465517	14.355866	-0.058992	4.783606
288.587511	7881.425444	14.360871	-0.059005	4.781240
288.692736	7873.373519	14.365875	-0.059020	4.778869
288.670229	7865.438116	14.370880	-0.059011	4.776532
288.369132	7857.434711	14.375885	-0.058949	4.774176
288.540776	7849.380843	14.380890	-0.058976	4.771801
288.314573	7841.386602	14.385895	-0.058929	4.769444
288.266788	7833.390470	14.390899	-0.058915	4.767085
288.455357	7825.396335	14.395904	-0.058945	4.764724
288.233390	7817.419471	14.400909	-0.058898	4.762369
288.178348	7809.363361	14.405914	-0.058883	4.759988
288.117450	7801.468524	14.410919	-0.058867	4.757654
287.924186	7793.330006	14.415923	-0.058825	4.755247
288.067191	7785.322385	14.420928	-0.058847	4.752877
287.864952	7777.300599	14.425933	-0.058804	4.750502
287.794826	7769.309858	14.430938	-0.058786	4.748135
287.882109	7761.369312	14.435943	-0.058797	4.745781
287.759483	7753.333294	14.440947	-0.058769	4.743398
287.811793	7745.377105	14.445952	-0.058774	4.741037
287.739657	7737.324565	14.450957	-0.058755	4.738647
287.657567	7729.331705	14.455962	-0.058735	4.736274
287.563896	7721.369020	14.460967	-0.058712	4.733908
287.510008	7713.290076	14.465971	-0.058697	4.731506
287.635980	7705.380935	14.470976	-0.058715	4.729153
287.473146	7697.298469	14.475981	-0.058680	4.726748
287.467488	7689.324584	14.480986	-0.058674	4.724374
287.820722	7681.380465	14.485991	-0.058734	4.722006
287.523616	7673.292176	14.490995	-0.058674	4.719596
287.600272	7665.370985	14.496000	-0.058683	4.717234
287.527927	7657.318370	14.501005	-0.058664	4.714831
287.443843	7649.273965	14.506010	-0.058644	4.712430
287.265779	7641.298651	14.511015	-0.058605	4.710049
287.114436	7633.316206	14.516019	-0.058572	4.707664
287.173299	7625.299062	14.521024	-0.058578	4.705267
287.219560	7617.356832	14.526029	-0.058581	4.702891
286.868059	7609.300436	14.531034	-0.058511	4.700481
287.003420	7601.366062	14.536039	-0.058531	4.698105
286.948798	7593.279892	14.541043	-0.058515	4.695682
286.847238	7585.325626	14.546048	-0.058491	4.693298
287.035023	7577.255961	14.551053	-0.058521	4.690878
286.922028	7569.312912	14.556058	-0.058495	4.688495
286.818110	7561.343869	14.561063	-0.058471	4.686103
286.629607	7553.267136	14.566067	-0.058430	4.683677
286.861427	7545.303595	14.571072	-0.058468	4.681284
286.574472	7537.316584	14.576077	-0.058410	4.678883
286.494870	7529.323771	14.581082	-0.058390	4.676478
286.513484	7521.234121	14.586087	-0.058388	4.674044
286.573599	7513.143768	14.591091	-0.058394	4.671607
286.534102	7505.212401	14.596096	-0.058382	4.669218
286.507421	7497.234459	14.601101	-0.058372	4.666813
286.457181	7489.228432	14.606106	-0.058357	4.664398
286.372475	7481.301893	14.611111	-0.058336	4.662006
286.374663	7473.189710	14.616115	-0.058331	4.659557
286.413698	7465.276240	14.621120	-0.058334	4.657167
286.173838	7457.239453	14.626125	-0.058284	4.654738
286.114034	7449.226398	14.631130	-0.058268	4.652315
286.209627	7441.201753	14.636135	-0.058280	4.649887
286.195472	7433.223066	14.641139	-0.058272	4.647472
286.140416	7425.260736	14.646144	-0.058257	4.645061
285.891414	7417.305918	14.651149	-0.058206	4.642650
285.876215	7409.191506	14.656154	-0.058198	4.640190
286.020813	7401.259989	14.661159	-0.058219	4.637784
285.933338	7393.211431	14.666163	-0.058198	4.635341
285.813402	7385.215363	14.671168	-0.058170	4.632913
285.792448	7377.180692	14.676173	-0.058161	4.630472
285.878469	7369.211154	14.681178	-0.058172	4.628050
285.790681	7361.169370	14.686183	-0.058151	4.625604
285.535916	7353.214558	14.691187	-0.058098	4.623183
285.315476	7345.183110	14.696192	-0.058052	4.620738
285.434596	7337.218170	14.701197	-0.058069	4.618312
285.391526	7329.177206	14.706202	-0.058056	4.615861
285.234948	7321.193575	14.711207	-0.058022	4.613427
285.148497	7313.136583	14.716211	-0.058000	4.610968
285.299139	7305.192600	14.721216	-0.058023	4.608543
285.315487	7297.173924	14.726221	-0.058021	4.606094
285.329566	7289.190152	14.731226	-0.058019	4.603654
285.297694	7281.198336	14.736231	-0.058008	4.601210
285.339830	7273.199598	14.741235	-0.058010	4.598763
285.155933	7265.191793	14.746240	-0.057971	4.596312
285.192931	7257.156763	14.751245	-0.057973	4.593852
285.118924	7249.092431	14.756250	-0.057954	4.591380
285.066676	7241.158710	14.761255	-0.057939	4.588948
284.932992	7233.101060	14.766259	-0.057909	4.586476
284.852241	7225.159641	14.771264	-0.057889	4.584039
284.710120	7217.147328	14.776269	-0.057857	4.581579
284.782956	7209.157430	14.781274	-0.057866	4.579124
284.874425	7201.143345	14.786279	-0.057877	4.576660
284.860033	7193.127616	14.791283	-0.057870	4.574195
284.588892	7185.120714	14.796288	-0.057814	4.571731
284.549364	7177.115779	14.801293	-0.057802	4.569266
284.532041	7169.114129	14.806298	-0.057793	4.566801
284.423056	7161.118035	14.811303	-0.057768	4.564336
284.274546	7153.112241	14.816307	-0.057735	4.561867
284.632290	7145.174232	14.821312	-0.057796	4.559417
284.573103	7137.164719	14.826317	-0.057780	4.556944
284.110589	7129.126466	14.831322	-0.057689	4.554461
284.171544	7121.110272	14.836327	-0.057695	4.551983
284.210051	7113.115661	14.841331	-0.057697	4.549511
284.229707	7105.095197	14.846336	-0.057696	4.547029
284.064650	7097.093935	14.851341	-0.057660	4.544552
284.152199	7089.144455	14.856346	-0.057671	4.542090
284.183506	7081.163244	14.861351	-0.057672	4.539616
284.032371	7073.159003	14.866355	-0.057639	4.537134
284.039560	7065.100135	14.871360	-0.057635	4.534633
283.961048	7057.095394	14.876365	-0.057615	4.532148
283.897435	7049.062853	14.881370	-0.057598	4.529653
283.761524	7041.117499	14.886375	-0.057568	4.527184
283.705035	7033.070721	14.891379	-0.057552	4.524681
283.807008	7025.177011	14.896384	-0.057566	4.522226
283.559018	7017.120140	14.901389	-0.057514	4.519717
283.725293	7009.155553	14.906394	-0.057540	4.517237
283.763739	7001.110946	14.911399	-0.057542	4.514730
283.442702	6993.011034	14.916403	-0.057477	4.512203
283.323012	6985.049523	14.921408	-0.057450	4.509719
283.498134	6977.057463	14.926413	-0.057477	4.507225
283.518819	6969.004890	14.931418	-0.057476	4.504710
283.243605	6961.128716	14.936423	-0.057420	4.502248
283.331821	6953.048670	14.941427	-0.057431	4.499721
283.230547	6945.095277	14.946432	-0.057407	4.497233
283.078454	6937.079925	14.951437	-0.057374	4.494723
283.079321	6929.045980	14.956442	-0.057369	4.492207
283.138763	6921.072836	14.961447	-0.057375	4.489708
282.991443	6913.078963	14.966451	-0.057342	4.487201
283.134665	6905.054317	14.971456	-0.057364	4.484684
283.239334	6897.086166	14.976461	-0.057378	4.482183
283.168880	6889.077287	14.981466	-0.057360	4.479667
283.063406	6881.096104	14.986471	-0.057335	4.477159
283.053307	6873.036173	14.991475	-0.057328	4.474624
282.894082	6865.037790	14.996480	-0.057293	4.472107
282.882278	6857.023714	15.001485	-0.057286	4.469585
282.814185	6849.043469	15.006490	-0.057268	4.467071
282.983533	6841.054461	15.011495	-0.057294	4.464553
282.908689	6833.049647	15.016499	-0.057275	4.462029
282.538787	6825.010947	15.021504	-0.057201	4.459491
282.498996	6817.043646	15.026509	-0.057189	4.456976
282.522201	6808.982363	15.031514	-0.057188	4.454430
282.375798	6801.033229	15.036519	-0.057155	4.451917
282.194260	6793.010089	15.041523	-0.057117	4.449379
282.356773	6785.035010	15.046528	-0.057142	4.446856
282.298980	6777.031479	15.051533	-0.057126	4.444322
282.270190	6769.064714	15.056538	-0.057115	4.441798
282.210329	6761.083177	15.061543	-0.057099	4.439268
282.128959	6753.026770	15.066547	-0.057079	4.436713
282.029735	6745.003791	15.071552	-0.057055	4.434166
281.963045	6736.967364	15.076557	-0.057037	4.431614
281.984500	6728.971801	15.081562	-0.057036	4.429074
282.057126	6720.959539	15.086567	-0.057045	4.426528
281.792015	6712.973996	15.091571	-0.056990	4.423987
281.811678	6705.018755	15.096576	-0.056989	4.421455
281.580674	6697.011693	15.101581	-0.056941	4.418905
281.630279	6688.967276	15.106586	-0.056945	4.416342
281.665690	6680.981562	15.111591	-0.056946	4.413796
281.470610	6672.957734	15.116595	-0.056905	4.411236
281.472524	6665.006222	15.121600	-0.056900	4.408698
281.316890	6656.969727	15.126605	-0.056866	4.406131
281.325620	6648.979510	15.131610	-0.056862	4.403577
281.335503	6640.974391	15.136615	-0.056859	4.401018
281.287990	6632.982608	15.141619	-0.056845	4.398461
281.473403	6625.022145	15.146624	-0.056874	4.395914
281.343038	6617.011703	15.151629	-0.056845	4.393347
281.335572	6608.940761	15.156634	-0.056838	4.390761
281.540117	6601.015256	15.161639	-0.056871	4.388221
281.404265	6592.955796	15.166643	-0.056841	4.385634
281.247523	6585.041488	15.171648	-0.056807	4.383092
281.265686	6576.990979	15.176653	-0.056805	4.380506
281.035839	6569.012492	15.181658	-0.056757	4.377941
281.164116	6561.021074	15.186663	-0.056776	4.375371
281.178840	6552.979998	15.191667	-0.056773	4.372784
281.100257	6544.995704	15.196672	-0.056754	4.370213
280.910029	6537.015197	15.201677	-0.056713	4.367640
280.867922	6528.923578	15.206682	-0.056700	4.365032
280.889252	6521.053392	15.211687	-0.056699	4.362493
280.872489	6512.981533	15.216691	-0.056691	4.359888
280.997941	6505.041415	15.221696	-0.056709	4.357324
280.711007	6496.995716	15.226701	-0.056650	4.354723
280.798761	6488.875550	15.231706	-0.056661	4.352098
280.962700	6480.919923	15.236711	-0.056687	4.349525
280.590771	6472.921322	15.241715	-0.056613	4.346933
280.598757	6464.941523	15.246720	-0.056609	4.344349
280.682926	6457.007366	15.251725	-0.056619	4.341778
280.596124	6448.960943	15.256730	-0.056598	4.339168
280.525955	6440.982555	15.261735	-0.056580	4.336578
280.487588	6432.930470	15.266739	-0.056568	4.333964
280.432912	6424.964293	15.271744	-0.056552	4.331375
280.399994	6416.941977	15.276749	-0.056541	4.328767
280.510218	6408.921564	15.281754	-0.056556	4.326159
280.362662	6401.032146	15.286759	-0.056524	4.323590
280.045663	6392.961294	15.291763	-0.056460	4.320959
280.055375	6384.982419	15.296768	-0.056456	4.318359
280.265873	6376.950449	15.301773	-0.056490	4.315742
280.044942	6368.917296	15.306778	-0.056444	4.313120
280.014456	6360.933728	15.311783	-0.056433	4.310513
279.910556	6352.906943	15.316787	-0.056409	4.307890
280.005769	6344.878765	15.321792	-0.056421	4.305267
279.903314	6336.970573	15.326797	-0.056397	4.302680
280.051401	6328.903212	15.331802	-0.056420	4.300040
279.832492	6320.988270	15.336807	-0.056374	4.297447
279.765606	6312.940401	15.341811	-0.056356	4.294810
279.617537	6304.943181	15.346816	-0.056323	4.292186
279.737093	6296.928489	15.351821	-0.056341	4.289558
279.453895	6288.915803	15.356826	-0.056283	4.286926
279.457959	6280.948842	15.361831	-0.056278	4.284309
279.475178	6272.928514	15.366835	-0.056276	4.281673
279.561364	6264.941829	15.371840	-0.056287	4.279047
279.293326	6256.946831	15.376845	-0.056232	4.276414
279.386480	6248.893033	15.381850	-0.056244	4.273763
279.248509	6240.884970	15.386855	-0.056214	4.271123
279.198051	6232.881631	15.391859	-0.056199	4.268484
279.018163	6224.895985	15.396864	-0.056161	4.265848
279.339525	6216.896040	15.401869	-0.056215	4.263210
279.252347	6208.897179	15.406874	-0.056194	4.260567
279.193695	6200.974358	15.411879	-0.056178	4.257948
279.089745	6192.917001	15.416883	-0.056153	4.255283
278.900051	6184.911310	15.421888	-0.056113	4.252632
278.944437	6176.868721	15.426893	-0.056116	4.249969
278.830494	6168.934263	15.431898	-0.056090	4.247339
278.950293	6160.917576	15.436903	-0.056107	4.244682
278.708605	6152.924055	15.441907	-0.056057	4.242028
278.726588	6144.924848	15.446912	-0.056055	4.239373
278.720147	6136.972661	15.451917	-0.056049	4.236731
278.645987	6128.929649	15.456922	-0.056030	4.234057
278.731159	6120.910807	15.461927	-0.056040	4.231391
278.661136	6112.913509	15.466931	-0.056022	4.228729
278.730709	6104.905181	15.471936	-0.056030	4.226063
278.698203	6096.930060	15.476941	-0.056019	4.223405
278.610804	6088.919421	15.481946	-0.055997	4.220733
278.642883	6080.979697	15.486951	-0.055998	4.218084
278.403667	6072.961164	15.491955	-0.055949	4.215405
278.318481	6064.954573	15.496960	-0.055928	4.212730
278.339544	6056.898654	15.501965	-0.055926	4.210037
278.223622	6048.961088	15.506970	-0.055900	4.207381
278.254540	6040.926329	15.511975	-0.055900	4.204692
278.278630	6032.986369	15.516979	-0.055900	4.202033
278.158467	6024.980328	15.521984	-0.055872	4.199348
278.021092	6016.966954	15.526989	-0.055841	4.196660
277.985317	6008.855243	15.531994	-0.055830	4.193937
278.130385	6000.804631	15.536999	-0.055851	4.191236
277.768658	5992.870442	15.542003	-0.055779	4.188566
277.653081	5984.886494	15.547008	-0.055752	4.185880
277.593989	5976.917096	15.552013	-0.055736	4.183199
277.647719	5968.876987	15.557018	-0.055741	4.180492
277.567673	5960.928751	15.562023	-0.055721	4.177814
277.552467	5952.883597	15.567027	-0.055713	4.175102
277.530060	5944.934592	15.572032	-0.055704	4.172421
277.414052	5936.864270	15.577037	-0.055677	4.169695
277.448952	5928.882182	15.582042	-0.055678	4.167000
277.362030	5920.907371	15.587047	-0.055657	4.164304
277.232405	5912.947473	15.592051	-0.055628	4.161610
277.276319	5904.964936	15.597056	-0.055631	4.158909
277.307084	5896.914277	15.602061	-0.055631	4.156184
277.110159	5888.870960	15.607066	-0.055590	4.153456
277.073282	5880.857102	15.612071	-0.055578	4.150738
277.036178	5872.863240	15.617075	-0.055566	4.148025
277.021711	5864.846286	15.622080	-0.055558	4.145303
276.861048	5856.936974	15.627085	-0.055523	4.142614
276.767455	5848.884603	15.632090	-0.055500	4.139876
276.890156	5840.914545	15.637095	-0.055518	4.137166
276.843428	5832.885867	15.642099	-0.055504	4.134432
276.675562	5824.885995	15.647104	-0.055468	4.131705
276.685429	5816.877918	15.652109	-0.055464	4.128976
276.699351	5808.871338	15.657114	-0.055462	4.126245
276.610549	5800.932225	15.662119	-0.055440	4.123534
276.574193	5792.896904	15.667123	-0.055428	4.120789
276.746835	5784.909685	15.672128	-0.055455	4.118061
276.673978	5776.883621	15.677133	-0.055436	4.115316
276.428808	5768.844579	15.682138	-0.055386	4.112561
276.558368	5760.875742	15.687143	-0.055405	4.109834
276.493106	5752.842789	15.692147	-0.055387	4.107080
276.357802	5744.851513	15.697152	-0.055357	4.104338
276.587363	5736.882138	15.702157	-0.055395	4.101607
276.350377	5728.899912	15.707162	-0.055345	4.098863
276.086368	5720.921425	15.712167	-0.055291	4.096118
276.031907	5712.871533	15.717171	-0.055276	4.093349
276.295771	5704.899432	15.722176	-0.055320	4.090610
276.320948	5696.910825	15.727181	-0.055319	4.087859
276.175570	5688.923240	15.732186	-0.055287	4.085106
276.230978	5680.987710	15.737191	-0.055292	4.082370
275.899618	5672.940341	15.742195	-0.055226	4.079590
275.864642	5664.982023	15.747200	-0.055214	4.076842
275.754911	5656.914568	15.752205	-0.055188	4.074053
275.740856	5648.892273	15.757210	-0.055181	4.071279
275.837330	5640.937862	15.762215	-0.055193	4.068529
275.697402	5632.905298	15.767219	-0.055162	4.065746
275.860978	5624.963524	15.772224	-0.055188	4.062997
275.655820	5616.937369	15.777229	-0.055144	4.060212
275.673569	5608.960041	15.782234	-0.055142	4.057445
275.688697	5600.930720	15.787239	-0.055140	4.054658
275.590726	5592.916899	15.792243	-0.055117	4.051873
275.617862	5584.899947	15.797248	-0.055117	4.049087
275.537399	5576.913551	15.802253	-0.055097	4.046308
275.377226	5568.969136	15.807258	-0.055062	4.043540
275.279704	5560.961343	15.812263	-0.055038	4.040749
275.272392	5552.943743	15.817267	-0.055032	4.037954
275.396918	5544.916361	15.822272	-0.055050	4.035156
275.257540	5536.831357	15.827277	-0.055019	4.032332
275.098592	5528.873527	15.832282	-0.054984	4.029550
275.048471	5520.893446	15.837287	-0.054970	4.026760
274.919905	5512.907983	15.842291	-0.054940	4.023965
274.887012	5504.916020	15.847296	-0.054929	4.021167
274.916968	5496.924270	15.852301	-0.054930	4.018368
274.817442	5488.905378	15.857306	-0.054906	4.015555
274.825288	5480.913306	15.862311	-0.054902	4.012752
274.604264	5472.869205	15.867315	-0.054856	4.009925
274.639625	5464.904970	15.872320	-0.054857	4.007128
274.763743	5456.904215	15.877325	-0.054875	4.004318
274.533460	5448.915781	15.882330	-0.054827	4.001504
274.563427	5440.965878	15.887335	-0.054828	3.998706
274.612046	5432.933877	15.892339	-0.054832	3.995878
274.819942	5424.911946	15.897344	-0.054865	3.993053
274.584065	5416.889860	15.902349	-0.054816	3.990220
274.516833	5408.903114	15.907354	-0.054799	3.987399
274.519116	5400.898588	15.912359	-0.054794	3.984572
274.331638	5392.941039	15.917363	-0.054754	3.981756
274.406933	5384.959569	15.922368	-0.054763	3.978933
274.390807	5376.967650	15.927373	-0.054755	3.976104
274.091847	5368.952167	15.932378	-0.054694	3.973260
274.200682	5360.931631	15.937383	-0.054709	3.970418
274.040952	5352.935422	15.942387	-0.054674	3.967578
273.941570	5344.920223	15.947392	-0.054650	3.964731
273.849802	5337.005343	15.952397	-0.054628	3.961918
274.017583	5328.969818	15.957402	-0.054654	3.959063
273.901771	5321.000776	15.962407	-0.054628	3.956226
273.808760	5312.961921	15.967411	-0.054605	3.953362
273.738245	5304.940130	15.972416	-0.054587	3.950503
273.822751	5296.939533	15.977421	-0.054598	3.947652
273.740119	5288.899355	15.982426	-0.054577	3.944781
273.561221	5280.990318	15.987431	-0.054539	3.941954
273.534195	5272.983623	15.992435	-0.054528	3.939092
273.535771	5265.001447	15.997440	-0.054524	3.936238
273.430463	5257.010223	16.002445	-0.054499	3.933376
273.533264	5248.962391	16.007450	-0.054513	3.930496
273.580104	5241.011994	16.012455	-0.054516	3.927647
273.206225	5233.016759	16.017459	-0.054442	3.924773
273.164530	5225.031958	16.022464	-0.054429	3.921907
273.276266	5216.998469	16.027469	-0.054444	3.919023
273.158332	5208.977110	16.032474	-0.054417	3.916138
273.082613	5200.975221	16.037479	-0.054398	3.913258
273.228813	5192.945552	16.042483	-0.054420	3.910370
273.185695	5185.000630	16.047488	-0.054407	3.907507
272.850215	5177.000202	16.052493	-0.054339	3.904617
272.691652	5169.007222	16.057498	-0.054305	3.901730
272.975782	5161.001066	16.062503	-0.054353	3.898845
272.654030	5152.970478	16.067507	-0.054288	3.895937
272.749064	5145.008287	16.072512	-0.054300	3.893060
272.750899	5136.967070	16.077517	-0.054295	3.890151
272.700878	5128.981104	16.082522	-0.054281	3.887258
272.631675	5121.003833	16.087527	-0.054263	3.884365
272.728008	5113.022164	16.092531	-0.054276	3.881473
272.663394	5105.021321	16.097536	-0.054259	3.878568
272.440731	5097.026239	16.102541	-0.054212	3.875659
272.504447	5088.790305	16.107546	-0.054218	3.872667
272.750357	5080.798128	16.112551	-0.054259	3.869764
272.332349	5072.888356	16.117555	-0.054176	3.866877
272.367658	5064.946741	16.122560	-0.054178	3.863984
272.233237	5056.979938	16.127565	-0.054148	3.861077
272.116372	5048.944696	16.132570	-0.054121	3.858143
271.987148	5040.975264	16.137575	-0.054091	3.855231
271.864601	5032.984226	16.142579	-0.054064	3.852308
272.010616	5024.962506	16.147584	-0.054086	3.849378
271.837777	5016.983868	16.152589	-0.054048	3.846454
271.839437	5008.992439	16.157594	-0.054043	3.843527
271.986946	5001.022920	16.162599	-0.054066	3.840609
271.867507	4993.019687	16.167603	-0.054038	3.837671
271.883245	4985.010903	16.172608	-0.054036	3.834731
271.932876	4977.019117	16.177613	-0.054040	3.831796
271.952165	4968.990993	16.182618	-0.054039	3.828845
271.775597	4961.022431	16.187623	-0.054001	3.825909
271.474967	4953.057715	16.192627	-0.053940	3.822970
271.605354	4945.062260	16.197632	-0.053959	3.820027
271.623242	4937.090282	16.202637	-0.053957	3.817087
271.352503	4929.080794	16.207642	-0.053902	3.814125
271.545335	4921.058850	16.212647	-0.053932	3.811166
271.378942	4913.057682	16.217651	-0.053896	3.808205
271.386194	4905.070572	16.222656	-0.053892	3.805250
271.455143	4897.120678	16.227661	-0.053900	3.802308
271.368583	4889.102509	16.232666	-0.053879	3.799336
271.334869	4881.143143	16.237671	-0.053867	3.796383
271.209046	4873.077613	16.242675	-0.053839	3.793388
271.274491	4865.051053	16.247680	-0.053846	3.790408
271.132789	4857.046264	16.252685	-0.053814	3.787429
270.852670	4849.097077	16.257690	-0.053757	3.784466
270.957313	4841.113971	16.262695	-0.053771	3.781497
270.875307	4833.104574	16.267699	-0.053751	3.778511
270.778375	4825.063098	16.272704	-0.053728	3.775510
270.793185	4817.087482	16.277709	-0.053725	3.772534
270.768700	4809.036106	16.282714	-0.053716	3.769527
270.609279	4801.116149	16.287719	-0.053681	3.766563
270.557770	4793.090895	16.292723	-0.053666	3.763560
270.627545	4785.114783	16.297728	-0.053674	3.760576
270.498327	4777.166174	16.302733	-0.053645	3.757595
270.403433	4769.118648	16.307738	-0.053622	3.754575
270.475776	4761.089919	16.312743	-0.053630	3.751564
270.392484	4753.096226	16.317747	-0.053610	3.748560
270.337262	4745.076543	16.322752	-0.053594	3.745545
270.445974	4737.143705	16.327757	-0.053610	3.742563
270.401756	4729.108861	16.332762	-0.053596	3.739537
270.152348	4721.195115	16.337767	-0.053545	3.736550
269.953597	4713.164665	16.342771	-0.053502	3.733517
270.165833	4705.107816	16.347776	-0.053537	3.730482
270.026588	4697.142176	16.352781	-0.053506	3.727470
269.775701	4689.149578	16.357786	-0.053454	3.724443
269.833333	4681.199485	16.362791	-0.053460	3.721437
269.989417	4673.182828	16.367795	-0.053483	3.718405
269.705359	4665.213643	16.372800	-0.053425	3.715379
269.845556	4657.080176	16.377805	-0.053446	3.712298
269.814880	4649.076095	16.382810	-0.053435	3.709259
269.545908	4641.138157	16.387815	-0.053380	3.706237
269.730931	4633.139187	16.392819	-0.053410	3.703201
269.689879	4625.150550	16.397824	-0.053397	3.700160
269.557042	4617.225222	16.402829	-0.053367	3.697139
269.436982	4609.219633	16.407834	-0.053340	3.694085
269.534671	4601.209893	16.412839	-0.053353	3.691032
269.262329	4593.209525	16.417843	-0.053297	3.687972
269.448945	4585.181937	16.422848	-0.053326	3.684909
269.249536	4577.257177	16.427853	-0.053284	3.681874
269.236304	4569.254268	16.432858	-0.053277	3.678811
269.145768	4561.256599	16.437863	-0.053255	3.675745
269.030600	4553.223312	16.442867	-0.053228	3.672663
269.088991	4545.213817	16.447872	-0.053234	3.669592
269.083608	4537.236369	16.452877	-0.053228	3.666528
268.850259	4529.225543	16.457882	-0.053179	3.663444
268.895879	4521.241906	16.462887	-0.053182	3.660374
268.897216	4513.230623	16.467891	-0.053177	3.657290
268.825434	4505.226961	16.472896	-0.053159	3.654205
268.827866	4497.239669	16.477901	-0.053154	3.651125
268.745265	4489.243028	16.482906	-0.053134	3.648037
268.830864	4481.214346	16.487911	-0.053145	3.644938
268.645187	4473.288371	16.492915	-0.053105	3.641869
268.925505	4465.271302	16.497920	-0.053152	3.638774
268.772914	4457.293715	16.502925	-0.053118	3.635681
268.772423	4449.220786	16.507930	-0.053113	3.632552
268.567636	4441.253318	16.512935	-0.053070	3.629456
268.522023	4433.227931	16.517939	-0.053056	3.626339
268.427580	4425.283516	16.522944	-0.053034	3.623250
268.251305	4417.298632	16.527949	-0.052996	3.620139
268.267456	4409.306530	16.532954	-0.052993	3.617029
268.302733	4401.321572	16.537959	-0.052995	3.613919
268.078190	4393.287190	16.542963	-0.052948	3.610780
268.168969	4385.328178	16.547968	-0.052960	3.607677
268.246721	4377.281021	16.552973	-0.052969	3.604536
267.978729	4369.325066	16.557978	-0.052914	3.601418
268.062222	4361.374434	16.562983	-0.052925	3.598309
268.152418	4353.342512	16.567987	-0.052936	3.595167
267.874524	4345.363619	16.572992	-0.052879	3.592031
267.906843	4337.355417	16.577997	-0.052880	3.588891
267.849962	4329.338331	16.583002	-0.052864	3.585741
267.807784	4321.401910	16.588007	-0.052851	3.582621
267.446572	4313.410440	16.593011	-0.052779	3.579468
267.528725	4305.430729	16.598016	-0.052789	3.576328
267.633399	4297.371627	16.603021	-0.052804	3.573156
267.629572	4289.353605	16.608026	-0.052798	3.569994
267.674077	4281.434055	16.613031	-0.052801	3.566869
267.580939	4273.424023	16.618035	-0.052778	3.563701
267.371923	4265.444608	16.623040	-0.052734	3.560540
267.290379	4257.467786	16.628045	-0.052714	3.557381
267.257378	4249.394489	16.633050	-0.052703	3.554182
267.213124	4241.347411	16.638055	-0.052689	3.550990
267.130688	4233.356016	16.643059	-0.052669	3.547816
267.033854	4225.383879	16.648064	-0.052646	3.544646
266.965835	4217.442688	16.653069	-0.052628	3.541487
266.937628	4209.421749	16.658074	-0.052618	3.538295
266.925965	4201.442093	16.663079	-0.052610	3.535116
266.955065	4193.418045	16.668083	-0.052611	3.531918
267.026982	4185.398830	16.673088	-0.052619	3.528721
266.928968	4177.441814	16.678093	-0.052595	3.525540
266.571579	4169.473307	16.683098	-0.052524	3.522344
266.854720	4161.488023	16.688103	-0.052571	3.519158
266.543110	4153.508888	16.693107	-0.052508	3.515953
266.448189	4145.484141	16.698112	-0.052485	3.512733
266.586757	4137.456814	16.703117	-0.052506	3.509517
266.633776	4129.455427	16.708122	-0.052510	3.506306
266.520377	4121.493032	16.713127	-0.052483	3.503102
266.487376	4113.486825	16.718131	-0.052472	3.499880
266.436234	4105.559152	16.723136	-0.052458	3.496686
266.384451	4097.537372	16.728141	-0.052443	3.493451
266.187561	4089.521885	16.733146	-0.052401	3.490212
266.339773	4081.555680	16.738151	-0.052424	3.487000
266.077238	4073.560234	16.743155	-0.052370	3.483760
265.981152	4065.584080	16.748160	-0.052347	3.480530
266.281824	4057.612165	16.753165	-0.052398	3.477312
266.182200	4049.576406	16.758170	-0.052374	3.474052
266.006223	4041.581151	16.763175	-0.052336	3.470803
266.036937	4033.552629	16.768179	-0.052337	3.467544
266.191653	4025.574850	16.773184	-0.052361	3.464306
265.906240	4017.626194	16.778189	-0.052302	3.461063
265.690197	4009.625987	16.783194	-0.052257	3.457799
265.931445	4001.610916	16.788199	-0.052297	3.454540
265.655454	3993.627641	16.793203	-0.052240	3.451274
265.687222	3985.642020	16.798208	-0.052241	3.448014
265.801921	3977.615321	16.803213	-0.052257	3.444737
265.567594	3969.659279	16.808218	-0.052209	3.441474
265.530214	3961.692019	16.813223	-0.052197	3.438210
265.417346	3953.660021	16.818227	-0.052170	3.434914
265.756347	3945.628197	16.823232	-0.052228	3.431629
265.546958	3937.642985	16.828237	-0.052184	3.428343
265.539222	3929.656759	16.833242	-0.052178	3.425059
265.437711	3921.718436	16.838247	-0.052154	3.421789
265.091168	3913.727428	16.843251	-0.052084	3.418486
265.042503	3905.713151	16.848256	-0.052070	3.415180
265.310311	3897.707199	16.853261	-0.052115	3.411885
265.125574	3889.692391	16.858266	-0.052075	3.408568
265.089838	3881.719246	16.863271	-0.052063	3.405270
264.995542	3873.770741	16.868275	-0.052041	3.401977
265.101519	3865.750902	16.873280	-0.052055	3.398658
264.861080	3857.811965	16.878285	-0.052005	3.395357
264.610989	3849.726816	16.883290	-0.051954	3.391993
264.901743	3841.714403	16.888295	-0.052003	3.388673
264.730723	3833.732507	16.893299	-0.051966	3.385347
264.607182	3825.778551	16.898304	-0.051937	3.382031
264.569978	3817.813236	16.903309	-0.051925	3.378711
264.413996	3809.808911	16.908314	-0.051891	3.375366
264.507295	3801.811021	16.913319	-0.051903	3.372030
264.342456	3793.792047	16.918323	-0.051868	3.368672
264.458122	3785.818557	16.923328	-0.051884	3.365340
264.384787	3777.846600	16.928333	-0.051865	3.361998
264.137140	3769.871382	16.933338	-0.051814	3.358646
264.182696	3761.891152	16.938343	-0.051817	3.355298
264.006178	3753.878418	16.943347	-0.051779	3.351926
263.880157	3745.869512	16.948352	-0.051751	3.348554
263.925287	3737.868875	16.953357	-0.051754	3.345187
264.199350	3729.872132	16.958362	-0.051800	3.341828
264.038624	3721.905995	16.963367	-0.051765	3.338462
263.797837	3713.894288	16.968371	-0.051715	3.335071
263.828809	3705.904229	16.973376	-0.051716	3.331695
263.885419	3697.917081	16.978381	-0.051721	3.328318
263.723309	3689.912101	16.983386	-0.051686	3.324922
263.743962	3681.988507	16.988391	-0.051684	3.321563
263.663781	3673.989084	16.993395	-0.051664	3.318166
263.452735	3666.005686	16.998400	-0.051620	3.314766
263.489433	3657.958939	17.003405	-0.051622	3.311346
263.531431	3649.932488	17.008410	-0.051624	3.307931
263.548484	3641.959713	17.013415	-0.051622	3.304534
263.504889	3633.993907	17.018419	-0.051609	3.301134
263.246351	3626.053904	17.023424	-0.051556	3.297734
263.335720	3618.033671	17.028429	-0.051567	3.294309
263.056602	3610.037743	17.033434	-0.051510	3.290877
263.236286	3602.059661	17.038439	-0.051539	3.287467
263.267714	3594.036798	17.043443	-0.051539	3.284028
263.252134	3586.083238	17.048448	-0.051531	3.280614
263.296465	3578.131142	17.053453	-0.051534	3.277198
263.173159	3570.087773	17.058458	-0.051506	3.273734
263.212586	3562.069478	17.063463	-0.051509	3.270283
262.949051	3554.120291	17.068467	-0.051454	3.266846
263.037893	3546.115891	17.073472	-0.051466	3.263396
262.945213	3538.132047	17.078477	-0.051443	3.259943
262.804677	3530.168275	17.083482	-0.051412	3.256494
262.796936	3522.153341	17.088487	-0.051406	3.253024
262.884887	3514.133910	17.093491	-0.051417	3.249553
262.839492	3506.166138	17.098496	-0.051403	3.246094
262.533571	3498.230767	17.103501	-0.051341	3.242636
262.509964	3490.205584	17.108506	-0.051332	3.239146
262.513660	3482.253948	17.113511	-0.051327	3.235686
262.352225	3474.175651	17.118515	-0.051292	3.232160
262.227151	3466.188026	17.123520	-0.051263	3.228671
262.201717	3458.198439	17.128525	-0.051254	3.225182
262.148881	3450.237904	17.133530	-0.051239	3.221700
262.249382	3442.263182	17.138535	-0.051252	3.218215
262.137957	3434.238456	17.143539	-0.051226	3.214695
262.122188	3426.249216	17.148544	-0.051218	3.211191
261.903568	3418.289122	17.153549	-0.051173	3.207687
261.927318	3410.311547	17.158554	-0.051172	3.204182
261.997693	3402.351074	17.163559	-0.051180	3.200683
261.645175	3394.368274	17.168563	-0.051109	3.197152
261.742012	3386.340019	17.173568	-0.051122	3.193616
261.902056	3378.329476	17.178573	-0.051147	3.190087
261.601849	3370.363584	17.183578	-0.051086	3.186554
261.585975	3362.381785	17.188583	-0.051077	3.183022
261.574129	3354.379588	17.193587	-0.051070	3.179477
261.640402	3346.393652	17.198592	-0.051077	3.175939
261.533488	3338.397289	17.203597	-0.051052	3.172385
261.385113	3330.397764	17.208602	-0.051020	3.168824
261.445130	3322.395026	17.213607	-0.051026	3.165266
261.276875	3314.461739	17.218611	-0.050989	3.161725
261.242332	3306.484655	17.223616	-0.050978	3.158167
261.414906	3298.472122	17.228621	-0.051005	3.154597
261.123532	3290.445037	17.233626	-0.050945	3.150997
261.165487	3282.468186	17.238631	-0.050948	3.147430
261.199853	3274.503884	17.243635	-0.050949	3.143864
261.044948	3266.528756	17.248640	-0.050915	3.140281
260.861690	3258.592681	17.253645	-0.050876	3.136710
261.050845	3250.550903	17.258650	-0.050906	3.133104
261.060302	3242.547673	17.263655	-0.050903	3.129503
260.819354	3234.574755	17.268659	-0.050853	3.125900
260.673772	3226.615614	17.273664	-0.050821	3.122304
260.806437	3218.620347	17.278669	-0.050840	3.118700
260.787220	3210.620950	17.283674	-0.050831	3.115083
260.711430	3202.639208	17.288679	-0.050812	3.111467
260.532762	3194.649435	17.293683	-0.050774	3.107838
260.704493	3186.623296	17.298688	-0.050801	3.104205
260.755833	3178.667220	17.303693	-0.050805	3.100594
260.455669	3170.719053	17.308698	-0.050744	3.096966
260.314313	3162.742564	17.313703	-0.050713	3.093328
260.139374	3154.727552	17.318707	-0.050675	3.089667
260.105949	3146.753071	17.323712	-0.050664	3.086027
260.112199	3138.760132	17.328717	-0.050660	3.082375
260.124280	3130.740607	17.333722	-0.050657	3.078707
260.052809	3122.797651	17.338727	-0.050638	3.075066
260.282182	3114.687442	17.343731	-0.050676	3.071358
260.022161	3106.737040	17.348736	-0.050622	3.067697
259.813876	3098.773369	17.353741	-0.050578	3.064027
259.766384	3090.798262	17.358746	-0.050564	3.060355
260.031588	3082.840200	17.363751	-0.050609	3.056701
259.699539	3074.847595	17.368755	-0.050542	3.052998
259.628889	3066.849629	17.373760	-0.050523	3.049301
259.900204	3058.859452	17.378765	-0.050569	3.045619
259.863171	3050.890212	17.383770	-0.050557	3.041928
259.564050	3042.965680	17.388775	-0.050496	3.038241
259.282370	3034.968452	17.393779	-0.050438	3.034516
259.382345	3026.927043	17.398784	-0.050452	3.030784
259.258571	3018.972268	17.403789	-0.050424	3.027078
259.185177	3010.987254	17.408794	-0.050405	3.023355
259.279843	3002.995348	17.413799	-0.050417	3.019632
259.131078	2995.032540	17.418803	-0.050385	3.015906
259.096046	2987.030435	17.423808	-0.050373	3.012163
259.300155	2979.020009	17.428813	-0.050406	3.008424
259.137229	2971.031180	17.433818	-0.050370	3.004671
259.045952	2963.118046	17.438823	-0.050348	3.000953
258.887962	2955.133453	17.443827	-0.050314	2.997194
258.898826	2947.110043	17.448832	-0.050311	2.993420
258.912363	2939.101102	17.453837	-0.050308	2.989648
258.688386	2931.114755	17.458842	-0.050261	2.985870
258.979520	2923.143646	17.463847	-0.050310	2.982120
258.862473	2915.175489	17.468851	-0.050283	2.978346
258.803619	2907.182983	17.473856	-0.050267	2.974559
258.718913	2899.204093	17.478861	-0.050246	2.970773
258.666094	2891.216251	17.483866	-0.050231	2.966978
258.689439	2883.264668	17.488871	-0.050231	2.963200
258.404423	2875.299784	17.493875	-0.050172	2.959396
258.371505	2867.315030	17.498880	-0.050161	2.955589
258.420898	2859.308865	17.503885	-0.050165	2.951772
258.232102	2851.308582	17.508890	-0.050125	2.947940
258.257592	2843.357698	17.513895	-0.050125	2.944138
258.016174	2835.361826	17.518899	-0.050075	2.940296
258.023276	2827.395222	17.523904	-0.050071	2.936476
257.924639	2819.399103	17.528909	-0.050047	2.932631
257.934349	2811.398532	17.533914	-0.050044	2.928784
258.023026	2803.418681	17.538919	-0.050055	2.924947
257.829733	2795.475409	17.543923	-0.050014	2.921107
257.978357	2787.486671	17.548928	-0.050037	2.917258
257.995541	2779.446592	17.553933	-0.050035	2.913372
257.931671	2771.397737	17.558938	-0.050018	2.909473
257.903780	2763.451030	17.563943	-0.050007	2.905620
257.913161	2755.484432	17.568947	-0.050004	2.901754
257.855962	2747.535769	17.573952	-0.049988	2.897888
257.801096	2739.564148	17.578957	-0.049973	2.894006
257.646267	2731.552183	17.583962	-0.049939	2.890093
257.762091	2723.585804	17.588967	-0.049956	2.886212
257.544034	2715.637047	17.593971	-0.049910	2.882317
257.623055	2707.661729	17.598976	-0.049919	2.878419
257.372669	2699.698125	17.603981	-0.049868	2.874503
257.185200	2691.692715	17.608986	-0.049828	2.870566
257.355083	2683.708066	17.613991	-0.049854	2.866652
257.259015	2675.726528	17.618995	-0.049831	2.862720
256.960777	2667.797001	17.624000	-0.049771	2.858798
256.922941	2659.802524	17.629005	-0.049758	2.854852
256.804555	2651.790275	17.634010	-0.049731	2.850887
256.812148	2643.817947	17.639015	-0.049727	2.846944
256.837049	2635.840854	17.644019	-0.049727	2.842993
256.743219	2627.878806	17.649024	-0.049704	2.839038
256.813043	2619.903743	17.654029	-0.049712	2.835081
256.400637	2611.905354	17.659034	-0.049630	2.831079
256.407626	2603.918502	17.664039	-0.049627	2.827100
256.604793	2595.908136	17.669043	-0.049658	2.823115
256.220793	2587.982645	17.674048	-0.049581	2.819134
256.383685	2579.996822	17.679053	-0.049607	2.815148
256.375660	2571.973250	17.684058	-0.049600	2.811128
256.503564	2564.005919	17.689063	-0.049619	2.807138
256.248321	2556.052790	17.694067	-0.049566	2.803128
256.051516	2548.102611	17.699072	-0.049524	2.799116
256.267168	2540.110297	17.704077	-0.049559	2.795101
256.092398	2532.106944	17.709082	-0.049522	2.791053
256.222242	2524.117181	17.714087	-0.049541	2.787023
256.266297	2516.131559	17.719091	-0.049544	2.782984
256.077979	2508.196727	17.724096	-0.049504	2.778952
255.868894	2500.251952	17.729101	-0.049460	2.774907
255.881803	2492.228019	17.734106	-0.049457	2.770830
255.914191	2484.267554	17.739111	-0.049458	2.766780
255.915908	2476.289868	17.744115	-0.049453	2.762713
255.694549	2468.334091	17.749120	-0.049407	2.758638
255.771801	2460.347326	17.754125	-0.049416	2.754559
255.658917	2452.275214	17.759130	-0.049390	2.750419
255.570769	2444.336514	17.764135	-0.049368	2.746343
255.473582	2436.382770	17.769139	-0.049345	2.742252
255.371600	2428.422103	17.774144	-0.049321	2.738151
255.184535	2420.458624	17.779149	-0.049281	2.734038
255.165245	2412.434803	17.784154	-0.049272	2.729897
255.323871	2404.477580	17.789159	-0.049297	2.725795
255.036974	2396.533813	17.794163	-0.049238	2.721667
255.054468	2388.554680	17.799168	-0.049236	2.717533
255.121773	2380.580550	17.804173	-0.049244	2.713398
255.030608	2372.575602	17.809178	-0.049222	2.709231
254.965115	2364.623696	17.814183	-0.049204	2.705087
254.822860	2356.657289	17.819187	-0.049173	2.700924
254.784420	2348.693206	17.824192	-0.049160	2.696762
254.887891	2340.708316	17.829197	-0.049175	2.692592
254.751639	2332.703190	17.834202	-0.049144	2.688390
254.890398	2324.756056	17.839207	-0.049165	2.684229
254.786936	2316.783860	17.844211	-0.049140	2.680033
254.762659	2308.830059	17.849216	-0.049131	2.675845
254.649888	2300.837875	17.854221	-0.049105	2.671625
254.364583	2292.850911	17.859226	-0.049046	2.667390
254.295202	2284.932016	17.864231	-0.049028	2.663197
254.063006	2276.943513	17.869235	-0.048980	2.658951
254.072570	2268.969657	17.874240	-0.048977	2.654722
254.058063	2260.971513	17.879245	-0.048969	2.650471
253.987492	2252.988359	17.884250	-0.048951	2.646217
254.114022	2245.032314	17.889255	-0.048969	2.641984
253.963647	2237.072600	17.894259	-0.048936	2.637724
253.862375	2229.103475	17.899264	-0.048912	2.633456
253.838664	2221.115381	17.904269	-0.048902	2.629175
253.809605	2213.120907	17.909274	-0.048892	2.624884
253.881315	2205.175860	17.914279	-0.048900	2.620619
253.810787	2197.217793	17.919283	-0.048882	2.616330
253.650966	2189.239879	17.924288	-0.048847	2.612018
253.801212	2181.251864	17.929293	-0.048870	2.607714
253.582301	2173.292730	17.934298	-0.048824	2.603393
253.613802	2165.346060	17.939303	-0.048825	2.599090
253.553825	2157.382529	17.944307	-0.048809	2.594763
253.510749	2149.216203	17.949312	-0.048795	2.590320
253.517861	2141.268992	17.954317	-0.048792	2.585992
253.390685	2133.342993	17.959322	-0.048763	2.581660
253.319457	2125.420515	17.964327	-0.048744	2.577326
253.162369	2117.492530	17.969331	-0.048710	2.572975
253.114514	2109.501466	17.974336	-0.048696	2.568590
252.925282	2101.565700	17.979341	-0.048656	2.564219
252.784502	2093.596654	17.984346	-0.048624	2.559825
252.883769	2085.652696	17.989351	-0.048638	2.555453
252.832993	2077.642908	17.994355	-0.048623	2.551028
252.501134	2069.715600	17.999360	-0.048556	2.546620
252.567578	2061.740483	18.004365	-0.048564	2.542207
252.597899	2053.756775	18.009370	-0.048564	2.537778
252.535235	2045.797675	18.014375	-0.048547	2.533349
252.433312	2037.804875	18.019379	-0.048523	2.528890
252.379237	2029.839137	18.024384	-0.048508	2.524443
252.402760	2021.904069	18.029389	-0.048507	2.520009
252.269338	2013.958720	18.034394	-0.048477	2.515552
252.199504	2005.967111	18.039399	-0.048459	2.511064
252.154134	1997.991960	18.044403	-0.048446	2.506580
251.996165	1990.031435	18.049408	-0.048411	2.502088
252.204962	1982.066325	18.054413	-0.048445	2.497611
252.127546	1974.085425	18.059418	-0.048425	2.493097
252.268316	1966.095000	18.064423	-0.048446	2.488586
252.200406	1958.159968	18.069427	-0.048429	2.484082
252.046035	1950.219526	18.074432	-0.048395	2.479560
251.885590	1942.292525	18.079437	-0.048360	2.475038
252.021288	1934.247008	18.084442	-0.048380	2.470461
252.100932	1926.303056	18.089447	-0.048390	2.465930
251.874363	1918.361185	18.094451	-0.048342	2.461369
251.711592	1910.432652	18.099456	-0.048307	2.456812
251.609621	1902.476228	18.104461	-0.048283	2.452235
251.657014	1894.472629	18.109466	-0.048287	2.447633
251.563084	1886.539075	18.114471	-0.048264	2.443052
251.346630	1878.611411	18.119475	-0.048219	2.438457
251.374115	1870.599669	18.124480	-0.048219	2.433823
251.365581	1862.571854	18.129485	-0.048212	2.429168
251.172275	1854.624844	18.134490	-0.048171	2.424537
251.311806	1846.666634	18.139495	-0.048192	2.419917
251.300607	1838.734084	18.144499	-0.048185	2.415290
251.217242	1830.753675	18.149504	-0.048164	2.410621
251.217029	1822.803327	18.154509	-0.048159	2.405968
251.006566	1814.870732	18.159514	-0.048114	2.401299
250.958725	1806.935527	18.164519	-0.048100	2.396632
250.803571	1798.963868	18.169523	-0.048066	2.391926
250.822910	1790.974155	18.174528	-0.048065	2.387214
250.864844	1783.010897	18.179533	-0.048068	2.382510
250.630162	1775.081353	18.184538	-0.048019	2.377795
250.689840	1767.130899	18.189543	-0.048025	2.373081
250.724982	1759.139427	18.194547	-0.048026	2.368332
250.395615	1751.226245	18.199552	-0.047960	2.363591
250.568818	1743.273583	18.204557	-0.047987	2.358857
250.545043	1735.288738	18.209562	-0.047977	2.354078
250.265651	1727.334034	18.214567	-0.047920	2.349286
250.226798	1719.375707	18.219571	-0.047908	2.344503
250.140490	1711.435134	18.224576	-0.047887	2.339716
250.228510	1703.470700	18.229581	-0.047898	2.334920
250.046962	1695.502881	18.234586	-0.047859	2.330089
250.135413	1687.542828	18.239591	-0.047871	2.325275
249.948241	1679.624859	18.244595	-0.047831	2.320454
249.804143	1671.690671	18.249600	-0.047799	2.315617
250.023451	1663.686733	18.254605	-0.047834	2.310757
249.782894	1655.736759	18.259610	-0.047784	2.305881
249.723032	1647.815210	18.264615	-0.047768	2.301028
249.811140	1639.841065	18.269619	-0.047780	2.296145
249.739579	1631.878569	18.274624	-0.047761	2.291244
249.443946	1623.975571	18.279629	-0.047701	2.286351
249.388354	1616.016745	18.284634	-0.047686	2.281434
249.415901	1608.077262	18.289639	-0.047686	2.276525
249.513794	1600.031735	18.294643	-0.047699	2.271545
249.320050	1592.090236	18.299648	-0.047657	2.266594
249.174819	1584.173020	18.304653	-0.047625	2.261652
249.062124	1576.226462	18.309658	-0.047599	2.256683
249.297921	1568.241893	18.314663	-0.047638	2.251710
249.174226	1560.301844	18.319667	-0.047610	2.246722
249.039155	1552.371154	18.324672	-0.047580	2.241728
249.017747	1544.451048	18.329677	-0.047571	2.236739
248.898339	1536.483955	18.334682	-0.047543	2.231701
248.968275	1528.514139	18.339687	-0.047551	2.226667
249.070213	1520.555593	18.344691	-0.047565	2.221631
248.938916	1512.639334	18.349696	-0.047535	2.216590
248.855815	1504.703304	18.354701	-0.047515	2.211529
248.731357	1496.756602	18.359706	-0.047487	2.206446
248.729519	1488.844185	18.364711	-0.047481	2.201384
248.535230	1480.908730	18.369715	-0.047440	2.196279
248.548657	1472.923735	18.374720	-0.047437	2.191148
248.576530	1464.973286	18.379725	-0.047437	2.186029
248.347795	1457.051400	18.384730	-0.047390	2.180893
248.354817	1449.122641	18.389735	-0.047386	2.175761
248.198991	1441.163563	18.394739	-0.047352	2.170583
248.054121	1433.225374	18.399744	-0.047320	2.165408
247.975648	1425.306854	18.404749	-0.047300	2.160238
247.780853	1417.388820	18.409754	-0.047259	2.155046
247.915881	1409.392259	18.414759	-0.047279	2.149821
248.013822	1401.422931	18.419763	-0.047292	2.144597
247.876220	1393.511584	18.424768	-0.047261	2.139376
247.798236	1385.595499	18.429773	-0.047242	2.134146
247.715707	1377.637996	18.434778	-0.047221	2.128874
247.730583	1369.710710	18.439783	-0.047219	2.123619
247.599444	1361.809234	18.444787	-0.047189	2.118354
247.539084	1353.835411	18.449792	-0.047173	2.113034
247.561860	1345.844274	18.454797	-0.047172	2.107697
247.298299	1337.932361	18.459802	-0.047118	2.102372
247.485310	1329.986687	18.464807	-0.047148	2.097055
247.303948	1322.062680	18.469811	-0.047109	2.091703
247.256782	1314.121836	18.474816	-0.047095	2.086339
247.277633	1306.209067	18.479821	-0.047094	2.080986
247.018310	1298.313671	18.484826	-0.047040	2.075604
246.830813	1290.391349	18.489831	-0.047000	2.070197
246.927755	1282.407944	18.494835	-0.047013	2.064762
247.056418	1274.463404	18.499840	-0.047032	2.059343
246.857208	1266.586643	18.504845	-0.046990	2.053922
246.695974	1258.638165	18.509850	-0.046955	2.048442
246.743383	1250.704925	18.514855	-0.046959	2.042979
246.750501	1242.786121	18.519859	-0.046955	2.037507
246.548279	1234.863964	18.524864	-0.046912	2.031997
246.510289	1226.921108	18.529869	-0.046900	2.026474
246.453690	1218.988107	18.534874	-0.046884	2.020941
246.301461	1211.094074	18.539879	-0.046851	2.015410
246.055306	1203.179157	18.544883	-0.046800	2.009839
246.027250	1195.235031	18.549888	-0.046790	2.004255
246.241962	1187.301664	18.554893	-0.046825	1.998689
246.071384	1179.380672	18.559898	-0.046788	1.993075
246.122517	1171.431382	18.564903	-0.046792	1.987448
245.988005	1163.535411	18.569907	-0.046762	1.981824
245.661173	1155.653797	18.574912	-0.046696	1.976174
245.872878	1147.688768	18.579917	-0.046730	1.970505
245.792252	1139.771579	18.584922	-0.046710	1.964823
245.647069	1131.893046	18.589927	-0.046678	1.959145
245.480741	1123.970538	18.594931	-0.046642	1.953416
245.599401	1115.964877	18.599936	-0.046659	1.947642
245.637738	1108.055925	18.604941	-0.046661	1.941911
245.338875	1100.170086	18.609946	-0.046600	1.936144
245.241717	1092.260755	18.614951	-0.046577	1.930365
245.186598	1084.339006	18.619955	-0.046562	1.924563
245.164948	1076.435687	18.624960	-0.046553	1.918761
245.299812	1068.501085	18.629965	-0.046573	1.912936
245.148317	1060.576985	18.634970	-0.046540	1.907069
245.022317	1052.696658	18.639975	-0.046511	1.901219
245.023410	1044.785107	18.644979	-0.046506	1.895343
244.968275	1036.860363	18.649984	-0.046491	1.889431
244.716369	1028.994278	18.654989	-0.046439	1.883523
244.585109	1021.104780	18.659994	-0.046409	1.877592
244.854218	1013.138923	18.664999	-0.046454	1.871631
244.711064	1005.227157	18.670003	-0.046423	1.865644
244.598304	997.336440	18.675008	-0.046397	1.859657
244.501962	989.455963	18.680013	-0.046374	1.853661
244.479300	981.520013	18.685018	-0.046364	1.847611
244.233585	973.666229	18.690023	-0.046314	1.841578
244.348671	965.746228	18.695027	-0.046330	1.835517
244.167604	957.850553	18.700032	-0.046291	1.829420
244.197727	949.945610	18.705037	-0.046292	1.823320
243.973647	942.070997	18.710042	-0.046245	1.817192
244.050814	934.146182	18.715047	-0.046254	1.811041
244.077111	926.234253	18.720051	-0.046254	1.804874
243.928603	918.377717	18.725056	-0.046221	1.798707
243.933477	910.456023	18.730061	-0.046217	1.792486
243.891334	902.517261	18.735066	-0.046204	1.786224
243.716871	894.665871	18.740071	-0.046167	1.779993
243.608645	886.782124	18.745075	-0.046141	1.773723
243.562972	878.878820	18.750080	-0.046128	1.767423
243.490735	871.019915	18.755085	-0.046109	1.761132
243.321606	863.156433	18.760090	-0.046073	1.754803
243.419157	855.223479	18.765095	-0.046086	1.748429
243.334612	847.355681	18.770099	-0.046065	1.742061
243.290447	839.477893	18.775104	-0.046052	1.735666
243.288027	831.597129	18.780109	-0.046046	1.729251
243.168408	823.719893	18.785114	-0.046019	1.722799
242.982059	815.888788	18.790119	-0.045979	1.716353
242.874002	807.986910	18.795123	-0.045954	1.709834
242.901610	800.082166	18.800128	-0.045954	1.703306
242.977823	792.205242	18.805133	-0.045963	1.696781
242.777621	784.342430	18.810138	-0.045921	1.690207
242.835241	776.463455	18.815143	-0.045927	1.683628
242.691317	768.621991	18.820147	-0.045895	1.677028
242.469135	760.758798	18.825152	-0.045848	1.670373
242.498181	752.884865	18.830157	-0.045849	1.663716
242.345800	745.034301	18.835162	-0.045815	1.657027
242.089089	737.201245	18.840167	-0.045762	1.650312
241.969274	729.342822	18.845171	-0.045735	1.643567
241.876769	721.481205	18.850176	-0.045713	1.636794
241.839295	713.578065	18.855181	-0.045701	1.629965
241.780827	705.692505	18.860186	-0.045685	1.623120
241.707065	697.857499	18.865191	-0.045666	1.616288
241.724746	689.982023	18.870195	-0.045664	1.609404
241.604084	682.141227	18.875200	-0.045637	1.602501
241.512210	674.323644	18.880205	-0.045615	1.595593
241.495129	666.440004	18.885210	-0.045606	1.588607
241.512924	658.591850	18.890215	-0.045605	1.581627
241.338347	650.780481	18.895219	-0.045567	1.574621
241.331705	642.915831	18.900224	-0.045561	1.567560
241.401331	635.072155	18.905229	-0.045569	1.560497
241.115527	627.279859	18.910234	-0.045511	1.553397
241.184320	619.404935	18.915239	-0.045518	1.546241
241.268953	611.555049	18.920243	-0.045529	1.539077
241.091840	603.742120	18.925248	-0.045491	1.531874
240.892174	595.935797	18.930253	-0.045449	1.524640
240.625778	588.152660	18.935258	-0.045394	1.517383
240.596263	580.310746	18.940263	-0.045384	1.510072
240.503317	572.485324	18.945267	-0.045362	1.502732
240.545037	564.657805	18.950272	-0.045364	1.495373
240.423833	556.851975	18.955277	-0.045337	1.487974
240.230129	549.056404	18.960282	-0.045296	1.480537
240.231934	541.233230	18.965287	-0.045291	1.473065
240.325526	533.361276	18.970291	-0.045303	1.465524
239.943442	525.614483	18.975296	-0.045227	1.457989
240.005845	517.791069	18.980301	-0.045234	1.450411
239.826242	510.000747	18.985306	-0.045195	1.442787
239.766068	502.228550	18.990311	-0.045179	1.435159
239.678703	494.417756	18.995315	-0.045158	1.427448
239.592703	486.636052	19.000320	-0.045137	1.419724
239.655242	478.841351	19.005325	-0.045144	1.411969
239.476070	471.070370	19.010330	-0.045105	1.404156
239.311521	463.327968	19.015335	-0.045070	1.396329
239.398658	455.496197	19.020339	-0.045081	1.388411
239.267450	447.726784	19.025344	-0.045051	1.380473
239.136788	439.988490	19.030349	-0.045022	1.372522
239.013545	432.211090	19.035354	-0.044994	1.364485
239.118655	424.446749	19.040359	-0.045009	1.356453
238.929871	416.689837	19.045363	-0.044969	1.348330
238.848683	408.940680	19.050368	-0.044949	1.340185
239.015107	401.165656	19.055373	-0.044975	1.332007
238.817667	393.434365	19.060378	-0.044933	1.323760
238.624680	385.733091	19.065383	-0.044892	1.315494
238.617096	377.853084	19.070387	-0.044885	1.307016
238.482322	370.144352	19.075392	-0.044855	1.298646
238.470363	362.421509	19.080397	-0.044848	1.290228
238.285094	354.723258	19.085402	-0.044809	1.281750
238.000866	347.057207	19.090407	-0.044751	1.273233
238.012516	339.325469	19.095411	-0.044748	1.264641
237.823967	331.643744	19.100416	-0.044708	1.256008
237.979277	323.908072	19.105421	-0.044732	1.247320
237.803744	316.242520	19.110426	-0.044694	1.238588
237.624617	308.563530	19.115431	-0.044656	1.229777
237.659429	300.845940	19.120435	-0.044658	1.220899
237.473516	293.189575	19.125440	-0.044618	1.211985
237.525317	285.506215	19.130445	-0.044623	1.203020
237.278898	277.876005	19.135450	-0.044572	1.193990
237.154057	270.218732	19.140455	-0.044544	1.184884
237.000522	262.585508	19.145459	-0.044511	1.175730
236.813082	254.946282	19.150464	-0.044471	1.166491
236.688649	247.336975	19.155469	-0.044443	1.157227
236.688905	239.634548	19.160474	-0.044438	1.147799
236.538217	232.033841	19.165479	-0.044405	1.138388
236.446653	224.412516	19.170483	-0.044383	1.128885
236.232848	216.828363	19.175488	-0.044338	1.119322
236.332577	209.201458	19.180493	-0.044352	1.109691
235.970846	201.649933	19.185498	-0.044280	1.099970
236.064474	194.044706	19.190503	-0.044292	1.090194
235.987152	186.478334	19.195507	-0.044273	1.080342
235.835366	178.921818	19.200512	-0.044240	1.070395
235.639934	171.388011	19.205517	-0.044199	1.060375
235.552185	163.836573	19.210522	-0.044177	1.050261
235.465755	156.312521	19.215527	-0.044157	1.040086
235.246147	148.814676	19.220531	-0.044111	1.029814
235.178816	141.298107	19.225536	-0.044094	1.019450
235.028669	133.819740	19.230541	-0.044061	1.009012
234.728070	126.369915	19.235546	-0.044000	0.998468
234.729037	118.853767	19.240551	-0.043995	0.987792
234.571701	111.400868	19.245555	-0.043961	0.977051
234.321511	103.972616	19.250560	-0.043910	0.966203
234.010279	96.589339	19.255565	-0.043847	0.955282
233.687051	89.197531	19.260570	-0.043782	0.944219
233.282031	81.850961	19.265575	-0.043702	0.933071
232.784591	74.524675	19.270579	-0.043605	0.921794
232.187972	67.226117	19.275584	-0.043489	0.910393
231.677159	60.157706	19.280589	-0.043390	0.899232