Tue Mar 23 11:49:52 2021

Number of Points = 3626
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.703773	-0.100152	0.000000	-0.000024	0.722560

0.694122	-0.187196	0.005005	-0.000022	0.722386
0.607622	-0.177017	0.010010	-0.000006	0.722376
0.754602	-0.199860	0.015014	-0.000034	0.722382
0.607265	-0.173565	0.020019	-0.000007	0.722383
0.473914	-0.151907	0.025024	0.000018	0.722379
0.494345	-0.151902	0.030029	0.000014	0.722386
0.362600	-0.132278	0.035034	0.000039	0.722379
0.334318	-0.124635	0.040038	0.000044	0.722384
0.539369	-0.161273	0.045043	0.000006	0.722384
0.593822	-0.173484	0.050048	-0.000005	0.722379
0.515468	-0.155656	0.055053	0.000010	0.722387
0.384857	-0.138101	0.060058	0.000034	0.722376
0.455471	-0.145799	0.065062	0.000021	0.722386
0.472732	-0.149482	0.070067	0.000018	0.722385
0.442319	-0.148771	0.075072	0.000023	0.722376
0.503455	-0.276680	0.080077	0.000012	0.722146
0.504703	-0.310523	0.085082	0.000011	0.722080
0.533439	-0.311681	0.090086	0.000006	0.722088
0.362960	-0.283610	0.095091	0.000038	0.722084
0.487807	-0.307877	0.100096	0.000014	0.722080
0.660066	-0.335539	0.105101	-0.000018	0.722086
0.478345	-0.356506	0.110106	0.000016	0.721981
0.404359	-0.458985	0.115110	0.000030	0.721754
0.613878	-0.494871	0.120115	-0.000010	0.721757
0.581022	-0.493126	0.125120	-0.000003	0.721749
0.699122	-0.510712	0.130125	-0.000026	0.721756
0.637854	-0.563975	0.135130	-0.000014	0.721630
0.676611	-0.663373	0.140134	-0.000021	0.721449
0.600239	-0.650148	0.145139	-0.000007	0.721448
0.446217	-0.626433	0.150144	0.000021	0.721441
0.621520	-0.696786	0.155149	-0.000011	0.721364
0.384774	-0.775148	0.160154	0.000033	0.721127
0.516454	-0.795949	0.165158	0.000008	0.721133
0.580374	-0.807978	0.170163	-0.000004	0.721132
0.427925	-0.850941	0.175168	0.000024	0.720994
0.459822	-0.908430	0.180173	0.000018	0.720892
0.247742	-0.875365	0.185178	0.000058	0.720883
0.371345	-0.910869	0.190182	0.000035	0.720857
0.389183	-1.069275	0.195187	0.000031	0.720551
0.303274	-1.056015	0.200192	0.000047	0.720547
0.413074	-1.071021	0.205197	0.000027	0.720556
0.335050	-1.211660	0.210202	0.000041	0.720252
0.455850	-1.243603	0.215206	0.000019	0.720232
0.522583	-1.260334	0.220211	0.000006	0.720223
0.575915	-1.434230	0.225216	-0.000004	0.719899
0.435850	-1.404672	0.230221	0.000022	0.719908
0.338923	-1.441284	0.235226	0.000040	0.719802
0.339875	-1.538546	0.240230	0.000040	0.719611
0.263102	-1.523941	0.245235	0.000054	0.719613
0.206717	-1.638512	0.250240	0.000064	0.719367
0.473795	-1.728977	0.255245	0.000015	0.719283
0.283461	-1.735774	0.260250	0.000050	0.719203
0.340846	-1.864323	0.265254	0.000039	0.718970
0.451098	-1.882111	0.270259	0.000019	0.718973
0.250417	-1.993294	0.275264	0.000056	0.718684
0.213345	-1.999477	0.280269	0.000063	0.718659
0.362842	-2.119202	0.285274	0.000035	0.718475
0.447481	-2.190171	0.290278	0.000019	0.718365
0.134487	-2.208420	0.295283	0.000077	0.718219
-0.002763	-2.282319	0.300288	0.000103	0.718025
0.015987	-2.324182	0.305293	0.000099	0.717949
0.122739	-2.463724	0.310298	0.000079	0.717711
0.014793	-2.472665	0.315302	0.000099	0.717655
0.085681	-2.619110	0.320307	0.000086	0.717391
-0.026695	-2.625474	0.325312	0.000107	0.717339
-1.877944	-2.416297	0.330317	0.000452	0.717101
-3.637606	-2.108814	0.335322	0.000779	0.717089
-4.099377	-2.033456	0.340326	0.000865	0.717076
-3.435458	-2.309051	0.345331	0.000741	0.716764
-4.421246	-2.137841	0.350336	0.000925	0.716756
-4.721205	-2.079626	0.355341	0.000980	0.716766
-4.035320	-2.256550	0.360346	0.000853	0.716657
-5.384473	-2.119747	0.365350	0.001104	0.716453
-5.384922	-2.117830	0.370355	0.001104	0.716456
-5.655803	-2.072085	0.375360	0.001154	0.716452
-5.298533	-2.131236	0.380365	0.001087	0.716461
-5.770420	-2.196216	0.385370	0.001175	0.716166
-6.475754	-2.082152	0.390374	0.001306	0.716143
-6.409425	-2.091145	0.395379	0.001294	0.716149
-6.174768	-2.138704	0.400384	0.001250	0.716138
-6.361126	-2.104268	0.405389	0.001285	0.716140
-6.889473	-2.136480	0.410394	0.001383	0.715890
-7.091509	-2.099134	0.415398	0.001420	0.715893
-7.238328	-2.072016	0.420403	0.001448	0.715895
-7.410506	-2.046130	0.425408	0.001480	0.715886
-6.867374	-2.138390	0.430413	0.001378	0.715895
-7.474745	-2.167738	0.435418	0.001491	0.715622
-8.562010	-2.008462	0.440422	0.001694	0.715554
-7.927609	-2.121390	0.445427	0.001576	0.715555
-8.157011	-2.084365	0.450432	0.001618	0.715547
-8.120992	-2.087922	0.455437	0.001611	0.715553
-8.290794	-2.060017	0.460442	0.001643	0.715549
-8.563020	-2.150125	0.465446	0.001694	0.715274
-9.374041	-2.023272	0.470451	0.001844	0.715239
-9.749219	-1.959217	0.475456	0.001914	0.715234
-8.775158	-2.127099	0.480461	0.001733	0.715245
-8.939204	-2.103245	0.485466	0.001763	0.715235
-9.239219	-2.048644	0.490470	0.001819	0.715237
-9.157305	-2.125160	0.495475	0.001804	0.715115
-10.343233	-2.017365	0.500480	0.002024	0.714909
-9.643474	-2.137575	0.505485	0.001894	0.714918
-10.215749	-2.039001	0.510490	0.002000	0.714912
-10.135154	-2.052979	0.515494	0.001985	0.714913
-9.654326	-2.136239	0.520499	0.001896	0.714918
-10.335860	-2.019344	0.525504	0.002022	0.714909
-10.181833	-2.162762	0.530509	0.001994	0.714679
-10.947910	-2.060281	0.535514	0.002136	0.714612
-11.059137	-2.040210	0.540518	0.002157	0.714612
-10.456433	-2.144710	0.545523	0.002044	0.714618
-10.688573	-2.107543	0.550528	0.002088	0.714610
-10.728472	-2.096678	0.555533	0.002095	0.714618
-11.084711	-2.094859	0.560538	0.002161	0.714496
-11.987662	-2.041843	0.565542	0.002329	0.714281
-11.379227	-2.149057	0.570547	0.002216	0.714284
-12.226409	-2.000407	0.575552	0.002373	0.714280
-11.873571	-2.058401	0.580557	0.002308	0.714290
-11.450009	-2.136299	0.585562	0.002229	0.714285
-12.010141	-2.037601	0.590566	0.002333	0.714283
-12.278982	-2.025710	0.595571	0.002383	0.714212
-12.937041	-2.027849	0.600576	0.002505	0.713975
-12.421958	-2.115022	0.605581	0.002409	0.713984
-13.115798	-1.995489	0.610586	0.002538	0.713976
-12.793172	-2.050892	0.615590	0.002478	0.713980
-12.780967	-2.051786	0.620595	0.002476	0.713983
-13.205707	-1.980933	0.625600	0.002555	0.713974
-12.707635	-2.065076	0.630605	0.002462	0.713983
-12.948356	-2.145519	0.635610	0.002507	0.713738
-13.937327	-2.007242	0.640614	0.002691	0.713663
-13.637784	-2.060811	0.645619	0.002635	0.713662
-13.566057	-2.079451	0.650624	0.002621	0.713651
-13.834314	-2.024578	0.655629	0.002671	0.713665
-13.978656	-2.003552	0.660634	0.002698	0.713656
-13.947746	-2.008289	0.665638	0.002692	0.713658
-13.630511	-2.131682	0.670643	0.002633	0.713525
-15.051275	-1.959900	0.675648	0.002897	0.713363
-14.639177	-2.028971	0.680653	0.002821	0.713372
-14.404021	-2.073975	0.685658	0.002777	0.713366
-14.803265	-2.003577	0.690662	0.002851	0.713365
-14.548534	-2.047950	0.695667	0.002803	0.713367
-14.564755	-2.047939	0.700672	0.002806	0.713362
-14.278793	-2.163263	0.705677	0.002753	0.713234
-15.652902	-2.021201	0.710682	0.003009	0.713029
-15.462610	-2.053312	0.715686	0.002973	0.713033
-15.461254	-2.051648	0.720691	0.002973	0.713037
-15.825926	-1.993484	0.725696	0.003041	0.713024
-15.207317	-2.095935	0.730701	0.002925	0.713039
-15.502782	-2.049119	0.735706	0.002980	0.713028
-15.326194	-2.139636	0.740710	0.002947	0.712911
-16.453201	-2.033897	0.745715	0.003157	0.712722
-16.481530	-2.031531	0.750720	0.003162	0.712717
-16.445661	-2.033665	0.755725	0.003155	0.712725
-16.607179	-2.010629	0.760730	0.003185	0.712714
-16.418359	-2.043067	0.765734	0.003150	0.712717
-16.087858	-2.101097	0.770739	0.003089	0.712718
-16.451964	-2.067170	0.775744	0.003156	0.712657
-17.333380	-2.041339	0.780749	0.003320	0.712396
-17.195760	-2.069436	0.785754	0.003295	0.712389
-17.388260	-2.033709	0.790758	0.003330	0.712392
-17.405581	-2.028993	0.795763	0.003333	0.712395
-17.711067	-1.979641	0.800768	0.003390	0.712385
-17.102284	-2.083409	0.805773	0.003277	0.712395
-17.128308	-2.081805	0.810778	0.003282	0.712389
-18.042688	-2.041080	0.815782	0.003452	0.712146
-18.404962	-2.001734	0.820787	0.003519	0.712096
-18.378120	-2.009899	0.825792	0.003514	0.712089
-18.042455	-2.065759	0.830797	0.003451	0.712097
-18.455460	-1.993528	0.835802	0.003528	0.712095
-18.339008	-2.015426	0.840806	0.003506	0.712093
-18.176341	-2.042032	0.845811	0.003476	0.712098
-18.228018	-2.093410	0.850816	0.003486	0.711977
-18.816253	-2.092513	0.855821	0.003595	0.711770
-19.101002	-2.047122	0.860826	0.003648	0.711760
-19.577218	-1.960379	0.865830	0.003736	0.711764
-19.027102	-2.055192	0.870835	0.003634	0.711770
-19.108502	-2.046342	0.875840	0.003649	0.711759
-19.461483	-1.977836	0.880845	0.003715	0.711770
-19.267212	-2.034221	0.885850	0.003678	0.711727
-19.708518	-2.090991	0.890854	0.003760	0.711457
-20.017672	-2.035733	0.895859	0.003818	0.711458
-20.651680	-1.926862	0.900864	0.003936	0.711450
-19.911513	-2.053895	0.905869	0.003798	0.711460
-20.113645	-2.021811	0.910874	0.003835	0.711452
-20.516530	-1.948758	0.915878	0.003910	0.711455
-20.189166	-2.004750	0.920883	0.003849	0.711460
-20.256730	-2.080303	0.925888	0.003862	0.711285
-21.215903	-1.978410	0.930893	0.004040	0.711147
-20.908195	-2.036220	0.935898	0.003983	0.711142
-21.157344	-1.990791	0.940902	0.004029	0.711144
-21.344281	-1.955624	0.945907	0.004064	0.711148
-21.176429	-1.989338	0.950912	0.004032	0.711140
-21.026517	-2.012387	0.955917	0.004005	0.711148
-21.097094	-2.016759	0.960922	0.004018	0.711114
-21.961182	-1.981662	0.965926	0.004178	0.710877
-21.394663	-2.081949	0.970931	0.004073	0.710879
-21.900560	-1.994019	0.975936	0.004167	0.710874
-21.834123	-2.000986	0.980941	0.004154	0.710884
-22.041973	-1.967917	0.985946	0.004193	0.710877
-21.808397	-2.010370	0.990950	0.004149	0.710875
-21.574016	-2.094197	0.995955	0.004106	0.710791
-23.179851	-1.938447	1.000960	0.004405	0.710531
-22.538962	-2.047924	1.005965	0.004285	0.710541
-22.823589	-2.000665	1.010970	0.004338	0.710534
-22.920560	-1.984615	1.015974	0.004356	0.710532
-22.629763	-2.031325	1.020979	0.004302	0.710542
-22.975046	-1.973688	1.025984	0.004366	0.710535
-22.907638	-1.981222	1.030989	0.004353	0.710544
-23.311269	-2.061838	1.035994	0.004428	0.710239
-23.639640	-2.013109	1.040998	0.004489	0.710220
-23.751004	-1.990275	1.046003	0.004510	0.710226
-23.904163	-1.966087	1.051008	0.004538	0.710220
-23.676311	-2.000492	1.056013	0.004496	0.710232
-23.616816	-2.015209	1.061018	0.004485	0.710224
-24.072815	-1.934758	1.066022	0.004570	0.710223
-23.972525	-2.053330	1.071027	0.004551	0.710022
-24.830024	-1.966053	1.076032	0.004710	0.709891
-24.634085	-1.996805	1.081037	0.004674	0.709900
-24.783033	-1.971491	1.086042	0.004701	0.709897
-24.607494	-2.003487	1.091046	0.004669	0.709896
-24.271118	-2.058716	1.096051	0.004606	0.709906
-24.942221	-1.943761	1.101056	0.004731	0.709897
-25.020565	-1.975321	1.106061	0.004745	0.709806
-25.591929	-1.977822	1.111066	0.004852	0.709597
-25.675925	-1.961857	1.116070	0.004867	0.709599
-25.645837	-1.965596	1.121075	0.004861	0.709603
-25.574463	-1.982425	1.126080	0.004848	0.709595
-25.547528	-1.982520	1.131085	0.004843	0.709604
-25.853329	-1.930896	1.136090	0.004900	0.709599
-25.718479	-1.955603	1.141094	0.004874	0.709598
-25.648094	-2.094142	1.146099	0.004861	0.709346
-26.859995	-1.919820	1.151104	0.005087	0.709263
-26.272482	-2.020703	1.156109	0.004977	0.709270
-25.909771	-2.087728	1.161114	0.004910	0.709266
-26.658387	-1.954545	1.166118	0.005049	0.709266
-26.565206	-1.968669	1.171123	0.005032	0.709271
-26.323702	-2.016007	1.176128	0.004987	0.709262
-26.727786	-2.077579	1.181133	0.005062	0.708995
-27.572441	-1.943572	1.186138	0.005219	0.708962
-27.438466	-1.967032	1.191142	0.005194	0.708963
-26.888443	-2.063421	1.196147	0.005091	0.708967
-27.476326	-1.962579	1.201152	0.005201	0.708959
-27.517413	-1.953948	1.206157	0.005208	0.708962
-27.099625	-2.028839	1.211162	0.005130	0.708961
-27.715848	-2.059445	1.216166	0.005245	0.708680
-28.358224	-1.961277	1.221171	0.005364	0.708648
-28.194368	-1.994893	1.226176	0.005334	0.708639
-27.678601	-2.081986	1.231181	0.005238	0.708649
-28.218518	-1.988947	1.236186	0.005338	0.708643
-28.365214	-1.963524	1.241190	0.005365	0.708641
-27.807300	-2.068489	1.246195	0.005261	0.708630
-28.996258	-1.994938	1.251200	0.005483	0.708353
-29.069581	-1.978345	1.256205	0.005496	0.708361
-29.016062	-1.991091	1.261210	0.005486	0.708354
-29.011596	-1.993889	1.266214	0.005485	0.708351
-29.128019	-1.969499	1.271219	0.005507	0.708358
-29.104241	-1.979787	1.276224	0.005502	0.708346
-28.785631	-2.032024	1.281229	0.005443	0.708355
-29.792101	-2.022225	1.286234	0.005630	0.708016
-30.067297	-1.974251	1.291238	0.005681	0.708014
-29.718908	-2.034094	1.296243	0.005616	0.708018
-30.078539	-1.974498	1.301248	0.005683	0.708010
-30.146987	-1.959281	1.306253	0.005696	0.708016
-29.904277	-2.004845	1.311258	0.005651	0.708011
-29.646461	-2.051311	1.316262	0.005602	0.708011
-30.381378	-2.059510	1.321267	0.005739	0.707732
-31.028487	-1.961207	1.326272	0.005860	0.707698
-30.841357	-1.989864	1.331277	0.005825	0.707707
-30.798936	-2.000163	1.336282	0.005817	0.707702
-31.093643	-1.948477	1.341286	0.005871	0.707700
-30.707092	-2.013490	1.346291	0.005799	0.707708
-30.838591	-1.994001	1.351296	0.005824	0.707701
-30.893703	-2.105353	1.356301	0.005834	0.707458
-31.706095	-1.998506	1.361306	0.005985	0.707382
-31.803542	-1.981973	1.366310	0.006003	0.707380
-31.726092	-1.993770	1.371315	0.005989	0.707385
-31.817935	-1.983095	1.376320	0.006006	0.707373
-31.588899	-2.019846	1.381325	0.005963	0.707382
-31.588471	-2.020755	1.386330	0.005963	0.707380
-32.252424	-2.026655	1.391334	0.006086	0.707131
-32.205968	-2.055823	1.396339	0.006077	0.707089
-32.485410	-2.008137	1.401344	0.006129	0.707085
-32.384266	-2.022720	1.406349	0.006110	0.707092
-32.342318	-2.031611	1.411354	0.006103	0.707090
-32.215027	-2.055129	1.416358	0.006079	0.707088
-32.180860	-2.122133	1.421363	0.006072	0.706966
-33.985269	-1.907379	1.426368	0.006408	0.706752
-33.210534	-2.041738	1.431373	0.006264	0.706759
-33.251729	-2.035695	1.436378	0.006271	0.706757
-33.410498	-2.008620	1.441382	0.006301	0.706755
-33.259550	-2.032974	1.446387	0.006273	0.706760
-33.528906	-1.988988	1.451392	0.006323	0.706752
-33.582335	-2.015103	1.456397	0.006333	0.706681
-34.373975	-1.990385	1.461402	0.006480	0.706447
-34.449903	-1.978577	1.466406	0.006494	0.706444
-34.553870	-1.956764	1.471411	0.006513	0.706450
-34.326977	-2.003198	1.476416	0.006471	0.706438
-33.921454	-2.070479	1.481421	0.006395	0.706449
-34.285666	-2.008186	1.486426	0.006463	0.706444
-34.770287	-1.923734	1.491430	0.006553	0.706440
-34.601621	-2.082504	1.496435	0.006522	0.706181
-35.056741	-2.027489	1.501440	0.006606	0.706129
-35.521828	-1.942247	1.506445	0.006693	0.706134
-35.179524	-2.005095	1.511450	0.006629	0.706130
-35.326831	-1.979905	1.516454	0.006656	0.706129
-35.293759	-1.982789	1.521459	0.006650	0.706135
-35.532391	-1.945009	1.526464	0.006694	0.706125
-35.551433	-2.017654	1.531469	0.006698	0.705973
-36.200431	-1.954999	1.536474	0.006818	0.705866
-36.145158	-1.965720	1.541478	0.006808	0.705865
-35.966804	-1.994654	1.546483	0.006775	0.705871
-36.270146	-1.944796	1.551488	0.006831	0.705862
-36.260751	-1.944896	1.556493	0.006829	0.705866
-35.986823	-1.995946	1.561498	0.006778	0.705861
-36.197376	-2.041952	1.566502	0.006817	0.705693
-37.324744	-1.921815	1.571507	0.007027	0.705531
-37.146965	-1.957784	1.576512	0.006994	0.705523
-36.944276	-1.991367	1.581517	0.006956	0.705528
-37.008209	-1.980415	1.586522	0.006968	0.705527
-37.131816	-1.959990	1.591526	0.006991	0.705524
-36.776423	-2.017960	1.596531	0.006925	0.705535
-36.830976	-2.076572	1.601536	0.006935	0.705398
-37.905070	-1.973217	1.606541	0.007134	0.705221
-37.555944	-2.037166	1.611546	0.007069	0.705217
-37.779632	-1.998049	1.616550	0.007111	0.705216
-37.618889	-2.023500	1.621555	0.007081	0.705223
-37.766896	-2.001283	1.626560	0.007108	0.705214
-37.759206	-1.999763	1.631565	0.007107	0.705221
-37.763247	-2.136548	1.636570	0.007108	0.704944
-38.721242	-1.991612	1.641574	0.007286	0.704892
-38.863555	-1.963318	1.646579	0.007312	0.704898
-38.599848	-2.015297	1.651584	0.007263	0.704888
-38.785185	-1.977088	1.656589	0.007297	0.704899
-38.895977	-1.960494	1.661594	0.007318	0.704893
-38.484801	-2.037442	1.666598	0.007241	0.704885
-39.095113	-2.070663	1.671603	0.007355	0.704599
-39.771473	-1.954381	1.676608	0.007481	0.704591
-39.485699	-2.000147	1.681613	0.007427	0.704602
-39.251387	-2.043671	1.686618	0.007384	0.704598
-39.894328	-1.931990	1.691622	0.007503	0.704593
-39.760632	-1.951811	1.696627	0.007478	0.704601
-39.477523	-2.007944	1.701632	0.007425	0.704590
-39.991218	-2.070553	1.706637	0.007521	0.704279
-40.928299	-1.911818	1.711642	0.007695	0.704262
-40.720223	-1.950743	1.716646	0.007656	0.704259
-39.989611	-2.076154	1.721651	0.007520	0.704269
-40.427176	-2.002432	1.726656	0.007602	0.704260
-40.229108	-2.033806	1.731661	0.007565	0.704269
-39.923972	-2.111126	1.736666	0.007508	0.704222
-41.037269	-2.045067	1.741670	0.007715	0.703956
-41.070602	-2.036202	1.746675	0.007721	0.703962
-41.229162	-2.011746	1.751680	0.007751	0.703954
-41.041258	-2.040808	1.756685	0.007716	0.703963
-41.247707	-2.005417	1.761690	0.007754	0.703961
-41.306026	-1.996702	1.766694	0.007765	0.703957
-41.084338	-2.112091	1.771699	0.007723	0.703805
-42.649381	-1.918439	1.776704	0.008015	0.703633
-42.158557	-2.001502	1.781709	0.007923	0.703642
-41.770962	-2.071075	1.786714	0.007851	0.703641
-42.219048	-1.993653	1.791718	0.007934	0.703636
-41.924719	-2.041534	1.796723	0.007879	0.703646
-42.109732	-2.012670	1.801728	0.007914	0.703637
-42.122959	-2.093184	1.806733	0.007916	0.703470
-43.361816	-1.933358	1.811738	0.008146	0.703347
-43.196624	-1.966726	1.816742	0.008116	0.703340
-42.589555	-2.071211	1.821747	0.008003	0.703347
-43.300838	-1.949264	1.826752	0.008135	0.703338
-43.138846	-1.973829	1.831757	0.008105	0.703347
-42.959481	-2.006284	1.836762	0.008071	0.703346
-43.132264	-2.050745	1.841766	0.008103	0.703194
-44.233521	-1.944123	1.846771	0.008308	0.703013
-43.863710	-2.015125	1.851776	0.008239	0.703003
-43.875430	-2.008880	1.856781	0.008241	0.703012
-44.090155	-1.970464	1.861786	0.008281	0.703012
-43.934962	-2.001778	1.866790	0.008252	0.703005
-43.763188	-2.028514	1.871795	0.008220	0.703013
-44.062528	-2.014301	1.876800	0.008276	0.702934
-44.834933	-1.991094	1.881805	0.008419	0.702703
-44.607635	-2.032866	1.886810	0.008377	0.702701
-45.013716	-1.961650	1.891814	0.008453	0.702698
-44.823858	-1.992539	1.896819	0.008417	0.702704
-44.832281	-1.998082	1.901824	0.008419	0.702690
-44.728569	-2.013151	1.906829	0.008399	0.702698
-45.047497	-1.972144	1.911834	0.008458	0.702666
-45.925228	-1.960757	1.916838	0.008622	0.702373
-45.277740	-2.071958	1.921843	0.008501	0.702381
-45.814637	-1.980043	1.926848	0.008601	0.702374
-45.885450	-1.966432	1.931853	0.008614	0.702376
-45.855665	-1.972531	1.936858	0.008608	0.702375
-45.809381	-1.983307	1.941862	0.008600	0.702370
-45.715957	-1.995772	1.946867	0.008582	0.702378
-46.246203	-2.020652	1.951872	0.008681	0.702137
-46.653095	-1.976215	1.956877	0.008756	0.702080
-46.379965	-2.025851	1.961882	0.008706	0.702079
-46.674891	-1.974871	1.966886	0.008760	0.702076
-46.714795	-1.962720	1.971891	0.008768	0.702086
-46.790874	-1.953726	1.976896	0.008782	0.702077
-46.462919	-2.008429	1.981901	0.008721	0.702085
-46.686992	-2.091271	1.986906	0.008762	0.701836
-47.701018	-1.956665	1.991910	0.008951	0.701743
-47.625852	-1.963451	1.996915	0.008937	0.701757
-47.637921	-1.965937	2.001920	0.008939	0.701748

-47.728280	-1.949514	2.011917	0.008956	0.701749
-47.463140	-1.997087	2.021914	0.008906	0.701748
-47.817095	-1.955791	2.031910	0.008972	0.701705
-48.336770	-1.982986	2.041907	0.009068	0.701462
-48.130852	-1.949911	2.051904	0.009030	0.701604
-48.131307	-1.898175	2.061901	0.009030	0.701709
-47.630526	-1.965560	2.071898	0.008936	0.701754
-47.559489	-1.978412	2.081894	0.008923	0.701754
-47.827786	-1.933741	2.091891	0.008973	0.701748
-47.701852	-1.957268	2.101888	0.008949	0.701746
-47.577077	-1.981053	2.111885	0.008925	0.701743
-47.528304	-1.988237	2.121882	0.008916	0.701747
-47.726564	-1.950647	2.131878	0.008953	0.701751
-47.466883	-1.963810	2.141875	0.008904	0.701819
-46.633783	-1.986236	2.151872	0.008749	0.702074
-46.518034	-2.007446	2.161869	0.008727	0.702074
-46.656856	-1.981031	2.171866	0.008753	0.702077
-46.514799	-2.006158	2.181862	0.008726	0.702078
-46.483917	-1.995435	2.191859	0.008720	0.702111
-46.012271	-1.951162	2.201856	0.008632	0.702371
-45.839078	-1.981684	2.211853	0.008600	0.702372
-45.787641	-1.990463	2.221850	0.008590	0.702374
-45.829300	-1.955399	2.231846	0.008598	0.702430
-44.879847	-1.993188	2.241843	0.008421	0.702696
-45.163612	-1.944645	2.251840	0.008473	0.702692
-44.971788	-1.978758	2.261837	0.008437	0.702693
-44.686155	-1.968967	2.271834	0.008384	0.702816
-44.069870	-1.981672	2.281830	0.008269	0.703013
-44.134980	-1.972845	2.291827	0.008281	0.703007
-44.440540	-1.917711	2.301824	0.008338	0.703009
-43.112886	-2.008171	2.311821	0.008090	0.703305
-43.255732	-1.962540	2.321818	0.008117	0.703346
-42.992955	-2.008797	2.331814	0.008068	0.703348
-43.255984	-1.958962	2.341811	0.008116	0.703354
-42.832699	-1.893008	2.351808	0.008037	0.703640
-42.343242	-1.981530	2.361805	0.007946	0.703638
-42.340670	-1.981518	2.371802	0.007945	0.703639
-41.946340	-1.952480	2.381798	0.007872	0.703840
-41.329108	-2.004246	2.391795	0.007757	0.703958
-41.595721	-1.956328	2.401792	0.007806	0.703959
-41.493538	-1.966208	2.411789	0.007787	0.703976
-40.947354	-1.920012	2.421786	0.007685	0.704266
-40.531549	-1.993542	2.431782	0.007607	0.704268
-40.777290	-1.948803	2.441779	0.007653	0.704270
-40.299435	-1.918043	2.451776	0.007564	0.704504
-39.703336	-1.979084	2.461773	0.007453	0.704595
-39.773651	-1.963560	2.471770	0.007465	0.704602
-39.618717	-1.967246	2.481766	0.007436	0.704650
-39.200618	-1.917738	2.491763	0.007358	0.704901
-38.900340	-1.974047	2.501760	0.007302	0.704896
-39.091616	-1.939947	2.511757	0.007338	0.704896
-38.579099	-1.895076	2.521754	0.007242	0.705171
-37.876701	-1.998649	2.531750	0.007111	0.705215
-38.188659	-1.942264	2.541747	0.007169	0.705217
-37.885153	-1.938098	2.551744	0.007112	0.705334
-36.974775	-2.004234	2.561741	0.006943	0.705528
-37.189364	-1.964622	2.571738	0.006982	0.705531
-37.131685	-1.974818	2.581734	0.006971	0.705532
-36.489687	-1.951648	2.591731	0.006852	0.705809
-36.505758	-1.921897	2.601728	0.006854	0.705864
-36.098490	-1.995139	2.611725	0.006778	0.705863
-36.327138	-1.914640	2.621722	0.006821	0.705943
-35.170050	-2.024614	2.631718	0.006605	0.706137
-35.467898	-1.972144	2.641715	0.006660	0.706136
-35.309764	-2.002070	2.651712	0.006631	0.706133
-35.008805	-1.941899	2.661709	0.006574	0.706362
-34.849835	-1.925866	2.671706	0.006545	0.706452
-34.915253	-1.909885	2.681702	0.006557	0.706461
-34.117787	-1.970308	2.691699	0.006408	0.706625
-33.792800	-1.958797	2.701696	0.006347	0.706765
-33.900586	-1.941603	2.711693	0.006367	0.706762
-33.720347	-1.962633	2.721690	0.006333	0.706784
-32.854569	-1.963472	2.731686	0.006172	0.707093
-32.926282	-1.951463	2.741683	0.006185	0.707092
-32.743459	-1.985361	2.751680	0.006151	0.707089
-32.581374	-1.935816	2.761677	0.006121	0.707247
-31.897098	-1.989980	2.771674	0.005993	0.707384
-31.934647	-1.984410	2.781670	0.006000	0.707382
-32.098166	-1.945763	2.791667	0.006030	0.707401
-31.183654	-1.958256	2.801664	0.005859	0.707704
-31.165600	-1.960610	2.811661	0.005856	0.707706
-30.955657	-1.998484	2.821658	0.005817	0.707705
-30.798393	-1.942863	2.831654	0.005787	0.707873
-30.204285	-1.977461	2.841651	0.005676	0.708017
-30.053846	-2.004886	2.851648	0.005648	0.708016
-30.332402	-1.953096	2.861645	0.005700	0.708021
-29.408334	-1.953696	2.871642	0.005528	0.708350
-29.239283	-1.981162	2.881638	0.005496	0.708356
-29.183045	-1.990202	2.891635	0.005485	0.708358
-29.039075	-1.961378	2.901632	0.005458	0.708468
-28.628777	-1.947552	2.911629	0.005382	0.708642
-28.454233	-1.977985	2.921626	0.005349	0.708644
-28.563538	-1.952298	2.931622	0.005369	0.708657
-27.581625	-1.974517	2.941619	0.005186	0.708963
-27.427135	-2.002428	2.951616	0.005157	0.708963
-27.779020	-1.939796	2.961613	0.005222	0.708963
-27.299474	-1.956668	2.971610	0.005133	0.709101
-26.721256	-1.973381	2.981606	0.005025	0.709274
-26.907130	-1.940644	2.991603	0.005059	0.709273
-26.822850	-1.931916	3.001600	0.005044	0.709321
-25.894030	-1.957016	3.011597	0.004870	0.709603
-25.685910	-1.994053	3.021594	0.004832	0.709603
-26.039214	-1.929764	3.031590	0.004897	0.709606
-25.446735	-1.938519	3.041587	0.004787	0.709800
-25.078815	-1.954520	3.051584	0.004718	0.709900
-25.128740	-1.945578	3.061581	0.004727	0.709900
-24.838125	-1.958780	3.071578	0.004673	0.709978
-24.149175	-1.956284	3.081574	0.004544	0.710228
-23.958958	-1.991458	3.091571	0.004509	0.710226
-24.035794	-1.977956	3.101568	0.004523	0.710226
-23.611787	-1.956208	3.111565	0.004444	0.710421
-23.158240	-1.979672	3.121562	0.004359	0.710536
-23.183162	-1.974715	3.131558	0.004363	0.710537
-22.738864	-2.053517	3.141555	0.004280	0.710539
-22.602391	-1.929937	3.151552	0.004255	0.710834
-22.193779	-1.981325	3.161549	0.004179	0.710877
-22.138610	-1.989503	3.171546	0.004168	0.710881
-22.246133	-1.928422	3.181542	0.004188	0.710965
-21.599590	-1.953064	3.191539	0.004067	0.711146
-21.586646	-1.957672	3.201536	0.004065	0.711142
-21.702633	-1.920987	3.211533	0.004086	0.711175
-20.815913	-1.937396	3.221530	0.003921	0.711457
-20.754692	-1.946180	3.231526	0.003909	0.711462
-20.663223	-1.961176	3.241523	0.003892	0.711465
-20.123903	-1.933222	3.251520	0.003791	0.711713
-19.755246	-1.971856	3.261517	0.003722	0.711767
-19.774738	-1.968845	3.271514	0.003726	0.711767
-19.763770	-1.910283	3.281510	0.003724	0.711888
-18.836498	-1.969556	3.291507	0.003551	0.712099
-18.862966	-1.964989	3.301504	0.003556	0.712099
-19.002995	-1.940152	3.311501	0.003581	0.712099
-18.204970	-1.945460	3.321498	0.003433	0.712373
-17.933724	-1.980713	3.331494	0.003382	0.712399
-18.115474	-1.949424	3.341491	0.003416	0.712397
-18.165304	-1.863577	3.351488	0.003425	0.712551
-17.100747	-1.967915	3.361485	0.003226	0.712721
-17.392044	-1.918761	3.371482	0.003280	0.712716
-17.199547	-1.931658	3.381478	0.003244	0.712759
-16.540399	-1.911497	3.391475	0.003121	0.713033
-16.292306	-1.957764	3.401472	0.003075	0.713030
-16.488243	-1.923205	3.411469	0.003111	0.713029
-15.713211	-1.929640	3.421466	0.002967	0.713292
-15.369989	-1.952713	3.431462	0.002903	0.713368
-15.391324	-1.948589	3.441459	0.002906	0.713369
-15.330959	-1.951086	3.451456	0.002895	0.713386
-14.554342	-1.953132	3.461453	0.002750	0.713657
-14.563168	-1.951079	3.471450	0.002752	0.713658
-14.606772	-1.942753	3.481446	0.002760	0.713660
-14.285967	-1.910050	3.491443	0.002700	0.713839
-13.913009	-1.906269	3.501440	0.002630	0.713979
-13.769036	-1.932260	3.511437	0.002603	0.713979
-13.745607	-1.899665	3.521434	0.002598	0.714052
-12.757646	-1.958804	3.531430	0.002414	0.714285
-12.731368	-1.962690	3.541427	0.002409	0.714287
-12.914641	-1.929799	3.551424	0.002443	0.714287
-12.246963	-1.929603	3.561421	0.002319	0.714525
-12.140167	-1.902856	3.571418	0.002298	0.714616
-11.818958	-1.960612	3.581414	0.002238	0.714615
-11.801274	-1.942188	3.591411	0.002235	0.714658
-11.200015	-1.918244	3.601408	0.002123	0.714919
-11.151006	-1.927791	3.611405	0.002113	0.714918
-11.052988	-1.945437	3.621402	0.002095	0.714918
-10.602978	-1.915610	3.631398	0.002011	0.715136
-10.135406	-1.946462	3.641395	0.001924	0.715241
-9.973820	-1.975431	3.651392	0.001894	0.715241
-10.246373	-1.915139	3.661389	0.001944	0.715264
-9.518419	-1.898706	3.671386	0.001808	0.715555
-8.942951	-2.000167	3.681382	0.001701	0.715557
-9.443960	-1.910885	3.691379	0.001794	0.715557
-8.898634	-1.910856	3.701376	0.001692	0.715750
-8.254224	-1.956044	3.711373	0.001572	0.715889
-7.780635	-2.039870	3.721370	0.001484	0.715890
-7.633086	-2.064483	3.731366	0.001456	0.715894
-7.803319	-1.991653	3.741363	0.001488	0.715978
-6.775548	-2.090775	3.751360	0.001296	0.716145
-7.018000	-2.050424	3.761357	0.001341	0.716140
-6.937112	-2.064545	3.771354	0.001326	0.716141
-6.565890	-2.124813	3.781350	0.001257	0.716153
-6.149826	-2.044423	3.791347	0.001179	0.716459
-5.691891	-2.127272	3.801344	0.001093	0.716457
-5.901991	-2.092054	3.811341	0.001132	0.716453
-6.110239	-2.054562	3.821338	0.001171	0.716454
-5.085428	-2.081846	3.831334	0.000980	0.716762
-5.141146	-2.070610	3.841331	0.000990	0.716765
-4.848260	-2.124222	3.851328	0.000935	0.716762
-5.148353	-2.051780	3.861325	0.000991	0.716800
-3.878661	-2.130056	3.871322	0.000754	0.717093
-4.012283	-2.105776	3.881318	0.000779	0.717095
-4.143491	-2.082557	3.891315	0.000803	0.717095
-3.991501	-2.083232	3.901312	0.000775	0.717147
-3.412830	-2.064326	3.911309	0.000667	0.717389
-3.097842	-2.121359	3.921306	0.000608	0.717388
-3.144915	-2.112136	3.931302	0.000617	0.717390
-2.983938	-2.047574	3.941299	0.000586	0.717574
-2.201627	-2.116247	3.951296	0.000441	0.717714
-2.431067	-2.076445	3.961293	0.000483	0.717713
-2.121494	-2.130576	3.971290	0.000425	0.717715
-1.731744	-2.056131	3.981286	0.000352	0.718000
-1.485518	-2.086206	3.991283	0.000306	0.718027
-1.540453	-2.077442	4.001280	0.000316	0.718026
-1.569728	-1.987062	4.011277	0.000322	0.718194
-1.240184	-1.960597	4.021274	0.000260	0.718363
-1.088415	-1.986149	4.031270	0.000232	0.718366
-1.075975	-1.901335	4.041267	0.000229	0.718538
-0.912694	-1.873009	4.051264	0.000198	0.718652
-1.023878	-1.836773	4.061261	0.000219	0.718685
-1.147351	-1.671056	4.071258	0.000242	0.718969
-0.976521	-1.690693	4.081254	0.000210	0.718991
-0.854459	-1.565148	4.091251	0.000187	0.719282
-0.756915	-1.558418	4.101248	0.000168	0.719330
-0.518067	-1.460176	4.111245	0.000124	0.719608
-0.500374	-1.418723	4.121242	0.000120	0.719696
-0.561335	-1.300296	4.131238	0.000131	0.719908
-0.618226	-1.184863	4.141235	0.000141	0.720116
-0.581832	-1.111519	4.151232	0.000134	0.720274
-0.618632	-0.967663	4.161229	0.000141	0.720545
-0.513483	-0.860343	4.171226	0.000121	0.720793
-0.502145	-0.767769	4.181222	0.000119	0.720980
-0.295019	-0.715113	4.191219	0.000080	0.721156
-0.221598	-0.581095	4.201216	0.000066	0.721446
-0.238062	-0.452639	4.211213	0.000069	0.721693
-0.184979	-0.330717	4.221210	0.000059	0.721952
-0.226106	-0.187559	4.231206	0.000066	0.722219
-0.081053	-0.074869	4.241203	0.000039	0.722491
-0.067909	0.071588	4.251200	0.000036	0.722784
0.000000	0.247793	4.261197	0.000023	0.723154

-0.061574	0.887098	4.266202	0.000034	0.724386
0.036272	2.128158	4.271206	0.000015	0.726847
0.051226	3.979107	4.276211	0.000011	0.730456
0.404000	6.323806	4.281216	-0.000057	0.735118
0.819781	9.159329	4.286221	-0.000136	0.740712
1.128309	12.509035	4.291226	-0.000196	0.747205
1.239295	16.341261	4.296230	-0.000219	0.754483
1.653085	20.519542	4.301235	-0.000299	0.762437
2.105277	25.102450	4.306240	-0.000386	0.771065
2.452475	30.058166	4.311245	-0.000454	0.780243
2.979757	35.342286	4.316250	-0.000556	0.789960
3.344256	40.968674	4.321254	-0.000627	0.800116
3.591280	46.914793	4.326259	-0.000677	0.810667
4.131555	53.096286	4.331264	-0.000782	0.821578
4.592272	59.562553	4.336269	-0.000872	0.832808
5.959500	66.094603	4.341274	-0.001131	0.844267
7.250595	72.889668	4.346278	-0.001376	0.855986
8.169672	79.950621	4.351283	-0.001552	0.867873
9.052781	87.223774	4.356288	-0.001721	0.879931
10.063089	94.638866	4.361293	-0.001914	0.892087
10.950077	102.256538	4.366298	-0.002084	0.904362
11.875990	110.016393	4.371302	-0.002262	0.916704
12.449037	117.945632	4.376307	-0.002374	0.929045
13.420608	125.937957	4.381312	-0.002560	0.941424
13.945043	134.105974	4.386317	-0.002663	0.953786
14.658744	142.319333	4.391322	-0.002802	0.966106
15.745648	150.563807	4.396326	-0.003009	0.978409
16.626303	158.910267	4.401331	-0.003179	0.990653
17.727420	167.280217	4.406336	-0.003390	1.002835
18.182428	175.793921	4.411341	-0.003480	1.014913
19.053374	184.279721	4.416346	-0.003648	1.026911
19.877067	192.817040	4.421350	-0.003807	1.038829
20.579495	201.391777	4.426355	-0.003943	1.050633
21.705533	209.936615	4.431360	-0.004159	1.062363
22.735086	218.528305	4.436365	-0.004356	1.074005
23.330651	227.182450	4.441370	-0.004473	1.085505
23.978208	235.851196	4.446374	-0.004599	1.096914
24.668104	244.497817	4.451379	-0.004733	1.108187
25.649630	253.122040	4.456384	-0.004922	1.119381
25.916981	261.847621	4.461389	-0.004977	1.130437
26.890806	270.457314	4.466394	-0.005164	1.141392
27.751964	279.109515	4.471398	-0.005330	1.152271
28.329350	287.759999	4.476403	-0.005444	1.162987
29.114215	296.375616	4.481408	-0.005595	1.173605
29.803750	304.976725	4.486413	-0.005729	1.184090
30.462309	313.597967	4.491418	-0.005858	1.194501
31.392526	322.140572	4.496422	-0.006037	1.204784
31.972201	330.748332	4.501427	-0.006150	1.214985
32.699078	339.319397	4.506432	-0.006291	1.225088
33.628590	347.859422	4.511437	-0.006470	1.235111
33.948398	356.457359	4.516442	-0.006535	1.245002
34.853957	364.963208	4.521446	-0.006710	1.254822
35.529282	373.468839	4.526451	-0.006841	1.264522
36.111283	382.007133	4.531456	-0.006955	1.274167
37.054385	390.442424	4.536461	-0.007136	1.283692
37.739855	398.939812	4.541466	-0.007269	1.293167
38.210823	407.450221	4.546470	-0.007363	1.302548
38.924420	415.982153	4.551475	-0.007501	1.311929
39.918978	424.415693	4.556480	-0.007692	1.321188
40.638184	432.833946	4.561485	-0.007832	1.330316
41.412471	441.234536	4.566490	-0.007981	1.339374
42.040885	449.643578	4.571494	-0.008104	1.348353
42.454268	458.081346	4.576499	-0.008187	1.357265
42.923791	466.482481	4.581504	-0.008280	1.366090
43.551859	474.860470	4.586509	-0.008402	1.374862
44.072960	483.250442	4.591514	-0.008505	1.383572
44.649546	491.637583	4.596518	-0.008618	1.392234
45.112747	499.990386	4.601523	-0.008709	1.400788
45.920417	508.304960	4.606528	-0.008865	1.409309
46.312402	516.682187	4.611533	-0.008944	1.417773
46.851637	525.007119	4.616538	-0.009050	1.426158
47.527393	533.333478	4.621542	-0.009181	1.434518
47.960863	541.657152	4.626547	-0.009267	1.442787
48.660627	549.954465	4.631552	-0.009403	1.451026
49.224530	558.263942	4.636557	-0.009514	1.459208
49.853611	566.551536	4.641562	-0.009636	1.467333
49.954367	574.981494	4.646566	-0.009661	1.475467
50.238819	583.266505	4.651571	-0.009719	1.483447
51.126937	591.483135	4.656576	-0.009890	1.491413
51.681336	599.743066	4.661581	-0.009999	1.499325
52.266626	608.002032	4.666586	-0.010113	1.507199
52.707033	616.302896	4.671590	-0.010201	1.515050
53.034653	624.574854	4.676595	-0.010267	1.522816
53.585238	632.830881	4.681600	-0.010375	1.530561
54.205681	641.062390	4.686605	-0.010496	1.538254
54.852173	649.283858	4.691610	-0.010622	1.545904
55.176898	657.591440	4.696614	-0.010688	1.553547
55.694734	665.799103	4.701619	-0.010790	1.561090
56.363548	674.015867	4.706624	-0.010920	1.568627
56.504885	682.300729	4.711629	-0.010952	1.576112
57.100741	690.502303	4.716634	-0.011068	1.583553
57.665823	698.719934	4.721638	-0.011179	1.590969
57.958191	706.975686	4.726643	-0.011239	1.598345
58.441378	715.186464	4.731648	-0.011334	1.605674
58.653336	723.448959	4.736653	-0.011379	1.612978
59.118074	731.648054	4.741658	-0.011471	1.620228
59.576788	739.859054	4.746662	-0.011562	1.627455
59.994087	748.116254	4.751667	-0.011645	1.634684
61.034809	756.210747	4.756672	-0.011844	1.641827
61.518915	764.391042	4.761677	-0.011940	1.648936
62.046077	772.590155	4.766682	-0.012043	1.656036
62.760909	780.741217	4.771686	-0.012182	1.663090
63.125583	788.960782	4.776691	-0.012255	1.670125
63.619545	797.160038	4.781696	-0.012353	1.677131
63.966215	805.353420	4.786701	-0.012423	1.684083
64.477495	813.546681	4.791706	-0.012523	1.691027
64.584226	821.785456	4.796710	-0.012548	1.697928
65.001614	829.953716	4.801715	-0.012632	1.704783
65.567229	838.139739	4.806720	-0.012742	1.711645
65.877100	846.324625	4.811725	-0.012806	1.718444
66.372312	854.466232	4.816730	-0.012903	1.725205
66.728295	862.661389	4.821734	-0.012975	1.731966
67.144957	870.820064	4.826739	-0.013058	1.738678
67.655662	878.962548	4.831744	-0.013158	1.745363
68.044764	887.132042	4.836749	-0.013236	1.752029
68.428903	895.299541	4.841754	-0.013313	1.758667
68.897307	903.433825	4.846758	-0.013406	1.765264
69.142903	911.621593	4.851763	-0.013457	1.771851
69.640505	919.776452	4.856768	-0.013555	1.778419
70.101786	927.904066	4.861773	-0.013646	1.784936
70.347043	936.121413	4.866778	-0.013697	1.791474
70.820417	944.285985	4.871782	-0.013791	1.797975
71.132941	952.410980	4.876787	-0.013855	1.804401
71.608097	960.547151	4.881792	-0.013948	1.810832
71.733511	968.726793	4.886797	-0.013977	1.817233
72.201520	976.842672	4.891802	-0.014070	1.823603
72.475114	985.001157	4.896806	-0.014126	1.829960
72.902961	993.122709	4.901811	-0.014211	1.836284
73.554365	1001.221950	4.906816	-0.014338	1.842596
74.055164	1009.337204	4.911821	-0.014436	1.848881
74.562065	1017.475746	4.916826	-0.014536	1.855163
75.080385	1025.599996	4.921830	-0.014638	1.861414
75.448567	1033.734407	4.926835	-0.014712	1.867635
75.826062	1041.926903	4.931840	-0.014788	1.873879
76.402477	1050.004490	4.936845	-0.014901	1.880039
76.769682	1058.133425	4.941850	-0.014974	1.886193
77.305416	1066.273285	4.946854	-0.015079	1.892355
77.600686	1074.415516	4.951859	-0.015140	1.898470
77.988520	1082.546972	4.956864	-0.015217	1.904569
78.129997	1090.712616	4.961869	-0.015249	1.910646
78.454411	1098.853543	4.966874	-0.015315	1.916705
78.916255	1106.953396	4.971878	-0.015406	1.922730
79.296469	1115.055653	4.976883	-0.015483	1.928729
79.639565	1123.211045	4.981888	-0.015552	1.934745
79.903740	1131.324609	4.986893	-0.015606	1.940702
80.573821	1139.383157	4.991898	-0.015737	1.946645
80.920063	1147.562159	4.996902	-0.015806	1.952622
81.174788	1155.682840	5.001907	-0.015859	1.958529
81.511272	1163.792238	5.006912	-0.015927	1.964418
81.885919	1171.874097	5.011917	-0.016002	1.970274
82.312819	1179.985628	5.016922	-0.016087	1.976140
82.676255	1188.098741	5.021926	-0.016160	1.981982
83.204280	1196.157962	5.026931	-0.016264	1.987786
83.622193	1204.307223	5.031936	-0.016347	1.993626
83.943459	1212.411953	5.036941	-0.016412	1.999406
84.204065	1220.506951	5.041946	-0.016466	2.005157
84.723644	1228.619522	5.046950	-0.016569	2.010930
84.943865	1236.748228	5.051955	-0.016615	2.016667
85.233260	1244.851059	5.056960	-0.016674	2.022377
85.724011	1252.936671	5.061965	-0.016771	2.028079
86.017655	1261.089013	5.066970	-0.016831	2.033791
86.192371	1269.205977	5.071974	-0.016869	2.039451
86.744999	1277.234538	5.076979	-0.016977	2.045072
87.451548	1285.300655	5.081984	-0.017114	2.050719
87.772486	1293.416720	5.086989	-0.017179	2.056346
87.909170	1301.548314	5.091994	-0.017210	2.061949
88.511016	1309.620419	5.096998	-0.017327	2.067543
88.720622	1317.752337	5.102003	-0.017372	2.073124
88.918781	1325.877986	5.107008	-0.017414	2.078684
89.265837	1333.947628	5.112013	-0.017484	2.084206
89.477955	1342.050463	5.117018	-0.017529	2.089722
89.835632	1350.182698	5.122022	-0.017601	2.095258
90.136197	1358.253019	5.127027	-0.017662	2.100732
90.459282	1366.348821	5.132032	-0.017728	2.106211
90.934475	1374.467324	5.137037	-0.017822	2.111706
91.343298	1382.573251	5.142042	-0.017903	2.117171
91.812282	1390.627659	5.147046	-0.017996	2.122594
92.113485	1398.693575	5.152051	-0.018057	2.127994
92.503090	1406.802137	5.157056	-0.018135	2.133417
92.801206	1414.872329	5.162061	-0.018196	2.138792
93.227490	1422.925813	5.167066	-0.018281	2.144155
93.495718	1431.036126	5.172070	-0.018336	2.149527
93.932950	1439.124301	5.177075	-0.018423	2.154887
94.025859	1447.240069	5.182080	-0.018446	2.160219
94.240383	1455.317832	5.187085	-0.018491	2.165525
94.581416	1463.386835	5.192090	-0.018560	2.170823
95.297129	1471.450756	5.197094	-0.018698	2.176140
95.411213	1479.551594	5.202099	-0.018725	2.181412
95.615236	1487.654102	5.207104	-0.018768	2.186681
95.909718	1495.770793	5.212109	-0.018829	2.191955
96.250485	1503.850566	5.217114	-0.018898	2.197196
96.649572	1511.908885	5.222118	-0.018977	2.202416
96.778309	1519.992269	5.227123	-0.019007	2.207615
97.394867	1528.050949	5.232128	-0.019127	2.212830
97.573497	1536.149917	5.237133	-0.019165	2.218020
97.719843	1544.230336	5.242138	-0.019198	2.223182
98.039415	1552.312065	5.247142	-0.019263	2.228349
98.699491	1560.356858	5.252147	-0.019391	2.233510
99.260047	1568.412652	5.257152	-0.019501	2.238657
100.011398	1576.401423	5.262157	-0.019646	2.243767
100.752738	1584.465922	5.267162	-0.019789	2.248912
100.838997	1592.632704	5.272166	-0.019811	2.254052
101.098113	1600.717218	5.277171	-0.019864	2.259144
101.614460	1608.787794	5.282176	-0.019966	2.264238
102.136011	1616.849917	5.287181	-0.020068	2.269315
102.363599	1625.036564	5.292186	-0.020116	2.274434
102.676117	1633.094061	5.297190	-0.020180	2.279467
103.090083	1641.117322	5.302195	-0.020262	2.284477
103.359756	1649.213195	5.307200	-0.020318	2.289509
103.646791	1657.298116	5.312205	-0.020377	2.294524
103.923016	1665.344829	5.317210	-0.020433	2.299504
104.180684	1673.423679	5.322214	-0.020487	2.304491
104.511205	1681.475863	5.327219	-0.020554	2.309457
105.030948	1689.568054	5.332224	-0.020656	2.314453
105.367113	1697.613298	5.337229	-0.020724	2.319393
105.637768	1705.662545	5.342234	-0.020779	2.324320
106.048471	1713.732909	5.347238	-0.020861	2.329262
106.513803	1721.805563	5.352243	-0.020953	2.334198
106.784896	1729.890729	5.357248	-0.021009	2.339115
106.939563	1737.972134	5.362253	-0.021043	2.344011
107.423420	1746.023220	5.367258	-0.021139	2.348904
107.706985	1754.150925	5.372262	-0.021197	2.353817
107.862472	1762.198295	5.377267	-0.021231	2.358662
108.285652	1770.253697	5.382272	-0.021315	2.363522
108.612794	1778.298373	5.387277	-0.021382	2.368359
108.996363	1786.381484	5.392282	-0.021458	2.373213
109.105002	1794.479137	5.397286	-0.021484	2.378043
109.413980	1802.520533	5.402291	-0.021547	2.382847
109.611317	1810.611723	5.407296	-0.021589	2.387661
109.896062	1818.669714	5.412301	-0.021647	2.392453
110.250133	1826.722662	5.417306	-0.021719	2.397237
110.643587	1834.773455	5.422310	-0.021797	2.402014
110.809011	1842.831774	5.427315	-0.021833	2.406768
111.273544	1850.896836	5.432320	-0.021925	2.411540
111.628467	1858.968165	5.437325	-0.021997	2.416297
111.677918	1867.050863	5.442330	-0.022011	2.421028
111.943787	1875.116573	5.447334	-0.022066	2.425756
112.470033	1883.158265	5.452339	-0.022169	2.430482
112.856862	1891.297997	5.457344	-0.022247	2.435244
113.003259	1899.332295	5.462349	-0.022279	2.439917
113.493063	1907.332741	5.467354	-0.022376	2.444588
113.755663	1915.411820	5.472358	-0.022430	2.449278
113.832021	1923.497609	5.477363	-0.022450	2.453949
114.229694	1931.544427	5.482368	-0.022529	2.458612
114.483778	1939.597781	5.487373	-0.022582	2.463260
114.655224	1947.660663	5.492378	-0.022619	2.467898
114.984738	1955.734933	5.497382	-0.022686	2.472546
115.202102	1963.796522	5.502387	-0.022732	2.477169
115.610965	1971.835084	5.507392	-0.022813	2.481785
115.672416	1979.898435	5.512397	-0.022830	2.486381
116.008349	1987.964934	5.517402	-0.022898	2.490990
116.257008	1996.048766	5.522406	-0.022949	2.495594
116.217614	2004.099253	5.527411	-0.022947	2.500149
116.711471	2012.128449	5.532416	-0.023045	2.504723
117.269890	2020.154937	5.537421	-0.023154	2.509291
117.310957	2028.289936	5.542426	-0.023167	2.513875
117.622691	2036.324282	5.547430	-0.023231	2.518414
117.926330	2044.332311	5.552435	-0.023292	2.522929
118.274656	2052.379868	5.557440	-0.023363	2.527461
118.468988	2060.461160	5.562445	-0.023404	2.531993
118.726120	2068.511835	5.567450	-0.023457	2.536503
119.110458	2076.558609	5.572454	-0.023534	2.541013
119.378452	2084.574836	5.577459	-0.023589	2.545490
119.760126	2092.656816	5.582464	-0.023666	2.550003
120.121866	2100.718944	5.587469	-0.023739	2.554495
120.440604	2108.746975	5.592474	-0.023803	2.558958
120.601623	2116.806558	5.597478	-0.023839	2.563419
120.854916	2124.857340	5.602483	-0.023891	2.567874
121.283350	2132.929226	5.607488	-0.023976	2.572345
121.347733	2141.019570	5.612493	-0.023994	2.576794
121.684371	2149.053085	5.617498	-0.024062	2.581222
122.049048	2157.103382	5.622502	-0.024135	2.585653
122.264245	2165.162942	5.627507	-0.024180	2.590072
122.551809	2173.418707	5.632512	-0.024239	2.594595
123.075589	2181.375339	5.637517	-0.024342	2.598963
123.158645	2189.388665	5.642522	-0.024363	2.603325
123.298671	2197.420512	5.647526	-0.024394	2.607694
123.561394	2205.445531	5.652531	-0.024449	2.612059
124.079765	2213.465524	5.657536	-0.024550	2.616432
124.269389	2221.522199	5.662541	-0.024591	2.620795
124.523565	2229.534328	5.667546	-0.024644	2.625131
124.999173	2237.597345	5.672550	-0.024738	2.629502
125.092774	2245.685833	5.677555	-0.024760	2.633854
125.204852	2253.727247	5.682560	-0.024787	2.638175
125.598683	2261.737779	5.687565	-0.024865	2.642491
125.736481	2269.795885	5.692570	-0.024896	2.646808
126.122477	2277.848348	5.697574	-0.024974	2.651132
126.538906	2285.899344	5.702579	-0.025056	2.655449
127.111708	2293.907080	5.707584	-0.025168	2.659746
127.174197	2301.977182	5.712589	-0.025185	2.664037
127.327875	2310.038082	5.717594	-0.025219	2.668322
127.795054	2318.133084	5.722598	-0.025312	2.672637
127.946393	2326.188616	5.727603	-0.025345	2.676905
128.062976	2334.234064	5.732608	-0.025372	2.681159
128.209311	2342.259722	5.737613	-0.025405	2.685397
128.624904	2350.265160	5.742618	-0.025488	2.689635
128.796698	2358.367491	5.747622	-0.025525	2.693901
129.008679	2366.395138	5.752627	-0.025570	2.698124
129.503622	2374.409372	5.757632	-0.025667	2.702351
129.811322	2382.439708	5.762637	-0.025730	2.706569
129.947160	2390.526613	5.767642	-0.025760	2.710798
130.348788	2398.581378	5.772646	-0.025841	2.715021
130.540426	2406.612651	5.777651	-0.025882	2.719211
130.885289	2414.631622	5.782656	-0.025951	2.723398
131.141834	2422.677828	5.787661	-0.026004	2.727588
131.299189	2430.739855	5.792666	-0.026039	2.731773
131.687817	2438.796081	5.797670	-0.026117	2.735963
131.939208	2446.832666	5.802675	-0.026169	2.740127
132.181446	2454.879679	5.807680	-0.026219	2.744291
132.388786	2462.931021	5.812685	-0.026263	2.748448
132.549121	2471.039712	5.817690	-0.026298	2.752625
132.875022	2479.117067	5.822694	-0.026364	2.756790
133.216584	2487.090978	5.827699	-0.026433	2.760896
133.332115	2495.133890	5.832704	-0.026460	2.765018
133.627673	2503.171559	5.837709	-0.026521	2.769142
133.988577	2511.207044	5.842714	-0.026593	2.773262
134.167498	2519.275223	5.847718	-0.026632	2.777382
134.269507	2527.311583	5.852723	-0.026656	2.781476
134.737358	2535.304565	5.857728	-0.026749	2.785562
134.851606	2543.369532	5.862733	-0.026775	2.789659
135.051158	2551.437817	5.867738	-0.026818	2.793756
135.432109	2559.479247	5.872742	-0.026894	2.797844
135.646062	2567.486270	5.877747	-0.026939	2.801898
135.861370	2575.543908	5.882752	-0.026985	2.805973
136.185066	2583.562484	5.887757	-0.027050	2.810028
136.333006	2591.638425	5.892762	-0.027083	2.814096
136.725919	2599.672020	5.897766	-0.027162	2.818151
136.797520	2607.713532	5.902771	-0.027180	2.822185
137.115076	2615.761076	5.907776	-0.027245	2.826231
137.366252	2623.810375	5.912781	-0.027297	2.830268
137.462909	2631.890095	5.917786	-0.027320	2.834306
137.800335	2639.904607	5.922790	-0.027388	2.838319
138.269246	2647.897586	5.927795	-0.027481	2.842323
138.510197	2655.949204	5.932800	-0.027531	2.846338
138.636723	2664.009480	5.937805	-0.027560	2.850344
138.819695	2672.072937	5.942810	-0.027599	2.854350
139.295179	2680.092897	5.947814	-0.027693	2.858345
139.631584	2688.099467	5.952819	-0.027761	2.862320
140.147035	2696.149251	5.957824	-0.027863	2.866321
140.597097	2704.160810	5.962829	-0.027952	2.870293
140.830787	2712.247206	5.967834	-0.028001	2.874285
141.048056	2720.302301	5.972838	-0.028046	2.878255
141.536817	2728.293922	5.977843	-0.028143	2.882203
141.645633	2736.354202	5.982848	-0.028168	2.886158
141.933821	2744.390432	5.987853	-0.028227	2.890107
142.143146	2752.443332	5.992858	-0.028272	2.894053
142.565988	2760.477398	5.997862	-0.028356	2.897996
142.679441	2768.522728	6.002867	-0.028382	2.901923
143.012557	2776.548466	6.007872	-0.028450	2.905847
143.294948	2784.597876	6.012877	-0.028507	2.909774
143.595179	2792.718807	6.017882	-0.028569	2.913732
143.775688	2800.748657	6.022886	-0.028608	2.917633
143.982442	2808.731638	6.027891	-0.028652	2.921508
144.272998	2816.772436	6.032896	-0.028711	2.925410
144.500330	2824.796708	6.037901	-0.028759	2.929296
144.815801	2832.840993	6.042906	-0.028823	2.933191
145.090610	2840.886277	6.047910	-0.028879	2.937079
145.057969	2848.927536	6.052915	-0.028878	2.940943
145.394294	2856.934339	6.057920	-0.028946	2.944806
145.673414	2864.986668	6.062925	-0.029004	2.948682
145.876669	2873.025943	6.067930	-0.029047	2.952542
146.402507	2881.086957	6.072934	-0.029150	2.956425
146.333609	2889.090458	6.077939	-0.029143	2.960244
146.825389	2897.110451	6.082944	-0.029240	2.964095
146.804567	2905.172909	6.087949	-0.029241	2.967935
147.037743	2913.215460	6.092954	-0.029290	2.971774
147.333070	2921.281656	6.097958	-0.029350	2.975622
147.491906	2929.272227	6.102963	-0.029385	2.979422
147.736560	2937.347709	6.107968	-0.029436	2.983261
148.066090	2945.346218	6.112973	-0.029503	2.987064
148.248523	2953.383845	6.117978	-0.029542	2.990873
148.586669	2961.465703	6.122982	-0.029610	2.994705
148.579648	2969.496347	6.127987	-0.029614	2.998492
148.956481	2977.494199	6.132992	-0.029690	3.002277
149.080326	2985.549446	6.137997	-0.029718	3.006072
149.438552	2993.537896	6.143002	-0.029790	3.009842
149.815068	3001.626541	6.148006	-0.029866	3.013655
149.954885	3009.646953	6.153011	-0.029897	3.017420
150.189017	3017.685679	6.158016	-0.029946	3.021193
150.632636	3025.678086	6.163021	-0.030034	3.024950
150.781482	3033.746005	6.168026	-0.030067	3.028723
151.012292	3041.816936	6.173030	-0.030115	3.032497
151.061836	3049.869121	6.178035	-0.030130	3.036249
151.398559	3057.863430	6.183040	-0.030198	3.039983
151.663376	3065.889266	6.188045	-0.030252	3.043723
151.870916	3073.916856	6.193050	-0.030296	3.047457
152.208211	3081.983595	6.198054	-0.030365	3.051211
152.188424	3090.046320	6.203059	-0.030366	3.054941
152.285705	3098.063696	6.208064	-0.030390	3.058651
152.778965	3106.068817	6.213069	-0.030487	3.062370
152.738563	3114.119193	6.218074	-0.030485	3.066080
152.975903	3122.147064	6.223078	-0.030534	3.069788
153.318528	3130.251542	6.228083	-0.030603	3.073531
153.636357	3138.292430	6.233088	-0.030668	3.077240
153.791504	3146.277892	6.238093	-0.030702	3.080911
154.058719	3154.258279	6.243098	-0.030757	3.084581
154.566746	3162.280770	6.248102	-0.030857	3.088276
154.652121	3170.346626	6.253107	-0.030878	3.091968
154.884039	3178.404090	6.258112	-0.030927	3.095658
155.215443	3186.425060	6.263117	-0.030994	3.099331
155.318996	3194.431798	6.268122	-0.031018	3.102983
155.656473	3202.472823	6.273126	-0.031087	3.106657
155.886129	3210.499192	6.278131	-0.031135	3.110315
156.068676	3218.575589	6.283136	-0.031174	3.113989
156.184593	3226.597934	6.288141	-0.031201	3.117632
156.396469	3234.625778	6.293146	-0.031246	3.121277
156.605130	3242.613713	6.298150	-0.031290	3.124899
156.840176	3250.653379	6.303155	-0.031339	3.128542
156.988894	3258.739391	6.308160	-0.031372	3.132198
157.313656	3266.760178	6.313165	-0.031438	3.135827
157.517324	3274.764098	6.318170	-0.031481	3.139440
157.674003	3282.820829	6.323174	-0.031516	3.143070
157.913080	3290.842779	6.328179	-0.031565	3.146683
158.267069	3298.874062	6.333184	-0.031637	3.150302
158.535530	3306.932812	6.338189	-0.031692	3.153925
158.655793	3314.967151	6.343194	-0.031720	3.157527
159.022973	3322.991093	6.348198	-0.031793	3.161130
159.360628	3330.947486	6.353203	-0.031862	3.164698
159.694531	3338.976419	6.358208	-0.031929	3.168294
159.775929	3347.063407	6.363213	-0.031950	3.171901
160.099277	3355.080339	6.368218	-0.032015	3.175483
160.365528	3363.115459	6.373222	-0.032070	3.179066
160.388021	3371.149258	6.378227	-0.032080	3.182634
160.514830	3379.203296	6.383232	-0.032109	3.186212
160.813528	3387.223347	6.388237	-0.032170	3.189778
161.005230	3395.273960	6.393242	-0.032211	3.193349
161.305292	3403.338281	6.398246	-0.032272	3.196927
161.569748	3411.306210	6.403251	-0.032326	3.200456
161.711793	3419.344880	6.408256	-0.032358	3.204008
162.012003	3427.378397	6.413261	-0.032419	3.207560
162.383926	3435.405734	6.418266	-0.032494	3.211108
162.635837	3443.458345	6.423270	-0.032546	3.214658
162.816145	3451.493241	6.428275	-0.032585	3.218194
163.196130	3459.492830	6.433280	-0.032661	3.221718
163.423869	3467.505547	6.438285	-0.032709	3.225238
163.460041	3475.572031	6.443290	-0.032721	3.228770
163.967028	3483.644514	6.448294	-0.032821	3.232320
164.174005	3491.705920	6.453299	-0.032865	3.235849
164.444888	3499.675107	6.458304	-0.032920	3.239336
164.379190	3507.714807	6.463309	-0.032913	3.242837
164.615604	3515.711756	6.468314	-0.032963	3.246327
165.006053	3523.734218	6.473318	-0.033041	3.249831
165.182370	3531.771444	6.478323	-0.033079	3.253329
165.574674	3539.795557	6.483328	-0.033157	3.256826
165.771939	3547.802277	6.488333	-0.033199	3.260304
165.925669	3555.829541	6.493338	-0.033233	3.263785
166.397570	3563.855408	6.498342	-0.033327	3.267274
166.474114	3571.910656	6.503347	-0.033346	3.270757
166.642400	3579.985802	6.508352	-0.033383	3.274249
166.853263	3588.003507	6.513357	-0.033427	3.277713
167.244754	3595.993995	6.518362	-0.033506	3.281169
167.441894	3604.014156	6.523366	-0.033548	3.284627
167.644839	3612.029994	6.528371	-0.033591	3.288079
167.739068	3620.077163	6.533376	-0.033614	3.291537
168.138197	3628.138480	6.538381	-0.033693	3.295009
168.209147	3636.164006	6.543386	-0.033712	3.298450
168.445351	3644.205933	6.548390	-0.033761	3.301900
168.638356	3652.220753	6.553395	-0.033802	3.305333
168.705816	3660.244115	6.558400	-0.033820	3.308761
169.073774	3668.288921	6.563405	-0.033894	3.312207
169.244330	3676.336909	6.568410	-0.033931	3.315643
169.550236	3684.348448	6.573414	-0.033994	3.319064
169.775680	3692.339453	6.578419	-0.034041	3.322471
169.979725	3700.355349	6.583424	-0.034084	3.325883
170.193748	3708.409631	6.588429	-0.034129	3.329309
170.232120	3716.450000	6.593434	-0.034142	3.332719
170.547524	3724.510021	6.598438	-0.034206	3.336144
170.754646	3732.499983	6.603443	-0.034250	3.339532
170.970773	3740.510692	6.608448	-0.034295	3.342925
171.061243	3748.576724	6.613453	-0.034318	3.346334
171.323043	3756.565954	6.618458	-0.034372	3.349712
171.552830	3764.633593	6.623462	-0.034420	3.353120
171.826448	3772.667218	6.628467	-0.034476	3.356511
172.118973	3780.665890	6.633472	-0.034536	3.359885
172.255741	3788.700134	6.638477	-0.034567	3.363264
172.311609	3796.730792	6.643482	-0.034582	3.366636
172.565210	3804.753528	6.648486	-0.034635	3.370008
172.763116	3812.794357	6.653491	-0.034677	3.373382
173.061786	3820.837082	6.658496	-0.034738	3.376757
173.154459	3828.853764	6.663501	-0.034761	3.380111
173.537527	3836.836878	6.668506	-0.034837	3.383458
173.940478	3844.895319	6.673510	-0.034918	3.386833
174.281085	3852.910233	6.678515	-0.034986	3.390184
174.354736	3861.058300	6.683520	-0.035006	3.393579
174.626769	3869.065872	6.688525	-0.035061	3.396918
174.812378	3877.011936	6.693530	-0.035101	3.400225
175.060516	3885.023877	6.698534	-0.035153	3.403559
175.213259	3893.075027	6.703539	-0.035187	3.406902
175.285596	3901.074427	6.708544	-0.035205	3.410218
175.630297	3909.113625	6.713549	-0.035275	3.413557
175.924639	3917.139301	6.718554	-0.035335	3.416884
176.216007	3925.139156	6.723558	-0.035395	3.420198
176.390086	3933.161024	6.728563	-0.035432	3.423514
176.465441	3941.200307	6.733568	-0.035452	3.426830
177.016440	3949.213360	6.738573	-0.035560	3.430148
177.103326	3957.266708	6.743578	-0.035581	3.433464
177.455071	3965.333095	6.748582	-0.035652	3.436790
177.730327	3973.310172	6.753587	-0.035709	3.440075
177.926250	3981.315093	6.758592	-0.035750	3.443365
178.333135	3989.349724	6.763597	-0.035831	3.446671
178.470662	3997.361935	6.768602	-0.035862	3.449955
178.680462	4005.462383	6.773606	-0.035907	3.453275
178.885290	4013.505388	6.778611	-0.035950	3.456568
178.916393	4021.511809	6.783616	-0.035961	3.459838
179.194864	4029.543759	6.788621	-0.036019	3.463122
179.402787	4037.536916	6.793626	-0.036063	3.466386
179.777399	4045.574451	6.798630	-0.036138	3.469670
180.116280	4053.625663	6.803635	-0.036206	3.472954
180.220557	4061.669236	6.808640	-0.036231	3.476226
180.523030	4069.651069	6.813645	-0.036293	3.479475
180.561959	4077.641049	6.818650	-0.036305	3.482716
180.830104	4085.696213	6.823654	-0.036360	3.485988
180.934169	4093.695417	6.828659	-0.036385	3.489229
181.058841	4101.776215	6.833664	-0.036414	3.492501
181.293854	4109.784230	6.838669	-0.036463	3.495743
181.509682	4117.771867	6.843674	-0.036508	3.498974
181.785076	4125.822060	6.848678	-0.036565	3.502229
181.907868	4133.800087	6.853683	-0.036593	3.505446
182.239776	4141.852555	6.858688	-0.036660	3.508698
182.613852	4149.908662	6.863693	-0.036735	3.511949
182.760132	4157.927543	6.868698	-0.036768	3.515175
182.986413	4165.956356	6.873702	-0.036815	3.518404
183.165479	4173.968189	6.878707	-0.036854	3.521622
183.490930	4181.915580	6.883712	-0.036920	3.524816
183.700157	4189.993017	6.888717	-0.036964	3.528055
183.746098	4198.037910	6.893722	-0.036978	3.531274
184.110658	4206.080384	6.898726	-0.037051	3.534498
184.154470	4214.119902	6.903731	-0.037065	3.537708
184.637797	4222.122262	6.908736	-0.037160	3.540914
184.954818	4230.142892	6.913741	-0.037224	3.544119
185.029553	4238.172411	6.918746	-0.037244	3.547317
185.377234	4246.213394	6.923750	-0.037314	3.550526
185.412393	4254.348524	6.928755	-0.037326	3.553759
185.558576	4262.372775	6.933760	-0.037358	3.556949
185.896787	4270.327225	6.938765	-0.037426	3.560114
186.130432	4278.306806	6.943770	-0.037475	3.563282
186.237508	4286.373836	6.948774	-0.037500	3.566479
186.640104	4294.339022	6.953779	-0.037581	3.569642
186.881234	4302.380867	6.958784	-0.037631	3.572827
186.955873	4310.441256	6.963789	-0.037650	3.576011
186.916148	4318.429238	6.968794	-0.037648	3.579162
187.284986	4326.466176	6.973798	-0.037722	3.582340
187.565614	4334.484236	6.978803	-0.037780	3.585505
187.754948	4342.485088	6.983808	-0.037820	3.588658
188.009773	4350.513824	6.988813	-0.037873	3.591822
188.235975	4358.535096	6.993818	-0.037920	3.594978
188.474000	4366.565875	6.998822	-0.037970	3.598136
188.607952	4374.577727	7.003827	-0.038000	3.601281
188.979160	4382.558381	7.008832	-0.038075	3.604417
189.034482	4390.629043	7.013837	-0.038090	3.607577
189.318730	4398.642025	7.018842	-0.038149	3.610718
189.556977	4406.710110	7.023846	-0.038198	3.613877
189.649763	4414.739507	7.028851	-0.038221	3.617014
189.759758	4422.721067	7.033856	-0.038247	3.620129
190.004161	4430.759550	7.038861	-0.038298	3.623268
190.340775	4438.751409	7.043866	-0.038366	3.626389
190.351659	4446.812128	7.048870	-0.038373	3.629525
190.532557	4454.854473	7.053875	-0.038412	3.632655
190.915159	4462.888399	7.058880	-0.038489	3.635785
191.059091	4470.889399	7.063885	-0.038521	3.638893
191.183717	4478.923607	7.068890	-0.038549	3.642010
191.468311	4486.908723	7.073894	-0.038608	3.645110
191.807106	4494.928575	7.078899	-0.038676	3.648223
191.889078	4502.982494	7.083904	-0.038697	3.651339
192.036330	4511.038128	7.088909	-0.038729	3.654455
192.476519	4519.048652	7.093914	-0.038817	3.657558
192.681138	4527.076303	7.098918	-0.038860	3.660659
192.640740	4535.065629	7.103923	-0.038858	3.663736
193.003158	4543.110271	7.108928	-0.038931	3.666843
193.051824	4551.136466	7.113933	-0.038945	3.669931
193.207775	4559.202979	7.118938	-0.038979	3.673036
193.409267	4567.229464	7.123942	-0.039022	3.676123
193.509059	4575.192158	7.128947	-0.039046	3.679181
193.849946	4583.220654	7.133952	-0.039115	3.682267
193.867721	4591.262517	7.138957	-0.039124	3.685348
194.187184	4599.229415	7.143962	-0.039188	3.688405
194.331090	4607.305156	7.148966	-0.039221	3.691497
194.327149	4615.316400	7.153971	-0.039225	3.694557
194.711812	4623.349253	7.158976	-0.039302	3.697633
194.879594	4631.351370	7.163981	-0.039339	3.700690
195.008782	4639.354471	7.168986	-0.039368	3.703743
195.509268	4647.387199	7.173990	-0.039467	3.706814
195.696050	4655.383652	7.178995	-0.039507	3.709861
195.820228	4663.486057	7.184000	-0.039535	3.712945
196.011300	4671.563058	7.189005	-0.039576	3.716017
196.308456	4679.477183	7.194010	-0.039637	3.719028
196.400474	4687.542579	7.199014	-0.039659	3.722089
196.771226	4695.470191	7.204019	-0.039733	3.725102
197.015159	4703.527012	7.209024	-0.039784	3.728158
197.105809	4711.563813	7.214029	-0.039806	3.731200
197.210267	4719.593141	7.219034	-0.039831	3.734238
197.415507	4727.664149	7.224038	-0.039875	3.737291
197.719279	4735.619054	7.229043	-0.039937	3.740300
198.197716	4743.607829	7.234048	-0.040031	3.743323
198.321099	4751.686473	7.239053	-0.040059	3.746370
198.538968	4759.689629	7.244058	-0.040105	3.749387
198.724518	4767.757777	7.249062	-0.040145	3.752426
198.851617	4775.796227	7.254067	-0.040174	3.755450
199.031492	4783.793933	7.259072	-0.040213	3.758458
199.381285	4791.815314	7.264077	-0.040283	3.761475
199.523077	4799.791704	7.269082	-0.040315	3.764469
199.599267	4807.861831	7.274086	-0.040335	3.767494
199.829296	4815.864179	7.279091	-0.040383	3.770494
200.001011	4823.929105	7.284096	-0.040420	3.773515
200.200212	4831.981388	7.289101	-0.040463	3.776528
200.425676	4839.918196	7.294106	-0.040510	3.779497
200.720042	4847.981997	7.299110	-0.040570	3.782512
200.839314	4855.988974	7.304115	-0.040598	3.785500
200.826872	4864.022652	7.309120	-0.040601	3.788493
201.311582	4872.037760	7.314125	-0.040696	3.791487
201.600179	4880.091866	7.319130	-0.040755	3.794488
201.883084	4888.103232	7.324134	-0.040813	3.797472
202.035243	4896.096648	7.329139	-0.040847	3.800443
202.239295	4904.091712	7.334144	-0.040890	3.803414
202.342791	4912.114920	7.339149	-0.040915	3.806391
202.729381	4920.102079	7.344154	-0.040992	3.809358
203.074841	4928.178994	7.349158	-0.041062	3.812355
203.161611	4936.212993	7.354163	-0.041083	3.815329
203.397129	4944.200068	7.359168	-0.041132	3.818285
203.661459	4952.237482	7.364173	-0.041187	3.821259
203.865022	4960.200069	7.369178	-0.041230	3.824202
204.007949	4968.290033	7.374182	-0.041262	3.827188
204.133579	4976.269522	7.379187	-0.041291	3.830130
204.320959	4984.319631	7.384192	-0.041331	3.833098
204.587795	4992.378440	7.389197	-0.041386	3.836067
204.720262	5000.305770	7.394202	-0.041416	3.838984
204.810894	5008.422626	7.399206	-0.041438	3.841967
205.311248	5016.358194	7.404211	-0.041537	3.844890
205.343524	5024.433853	7.409216	-0.041548	3.847852
205.520398	5032.480581	7.414221	-0.041586	3.850804
205.724584	5040.474933	7.419226	-0.041630	3.853735
205.951367	5048.539971	7.424230	-0.041677	3.856690
206.154915	5056.484414	7.429235	-0.041720	3.859599
206.252870	5064.544933	7.434240	-0.041744	3.862545
206.326534	5072.554781	7.439245	-0.041763	3.865471
206.383641	5080.587033	7.444250	-0.041779	3.868402
206.748535	5088.650146	7.449254	-0.041852	3.871348
206.928320	5096.860598	7.454259	-0.041891	3.874341
206.987807	5104.845260	7.459264	-0.041908	3.877248
207.302526	5112.752935	7.464269	-0.041971	3.880130
207.566458	5120.732040	7.469274	-0.042026	3.883034
207.723446	5128.734014	7.474278	-0.042060	3.885943
207.870633	5136.752037	7.479283	-0.042093	3.888855
208.132468	5144.761577	7.484288	-0.042147	3.891763
208.398016	5152.795142	7.489293	-0.042202	3.894679
208.559703	5160.813452	7.494298	-0.042237	3.897584
208.674929	5168.812577	7.499302	-0.042264	3.900480
209.035533	5176.832812	7.504307	-0.042337	3.903386
209.061661	5184.845950	7.509312	-0.042347	3.906280
209.312018	5192.904735	7.514317	-0.042399	3.909194
209.614479	5200.912457	7.519322	-0.042460	3.912087
209.982497	5208.962812	7.524326	-0.042534	3.914995
209.850749	5216.969781	7.529331	-0.042515	3.917876
210.008026	5224.945598	7.534336	-0.042550	3.920749
210.309821	5232.993981	7.539341	-0.042611	3.923648
210.490708	5240.968391	7.544346	-0.042650	3.926517
210.881922	5249.007929	7.549350	-0.042728	3.929410
211.026365	5257.072659	7.554355	-0.042761	3.932306
211.049532	5265.041318	7.559360	-0.042770	3.935163
211.327656	5273.100996	7.564365	-0.042827	3.938055
211.726145	5281.060553	7.569370	-0.042907	3.940912
211.919933	5289.083979	7.574374	-0.042948	3.943785
211.799857	5297.139821	7.579379	-0.042931	3.946663
212.021635	5305.152751	7.584384	-0.042978	3.949529
212.285515	5313.217718	7.589389	-0.043032	3.952412
212.389165	5321.230644	7.594394	-0.043057	3.955272
212.672513	5329.257557	7.599398	-0.043115	3.958137
212.979001	5337.222679	7.604403	-0.043177	3.960979
213.143015	5345.204740	7.609408	-0.043213	3.963823
213.423192	5353.261821	7.614413	-0.043271	3.966693
213.642616	5361.236298	7.619418	-0.043317	3.969531
213.936073	5369.309008	7.624422	-0.043377	3.972402
214.160227	5377.331927	7.629427	-0.043424	3.975253
214.349139	5385.326219	7.634432	-0.043465	3.978091
214.469816	5393.392010	7.639437	-0.043492	3.980951
214.418039	5401.342752	7.644442	-0.043488	3.983765
214.866343	5409.411437	7.649446	-0.043577	3.986628
215.002737	5417.403061	7.654451	-0.043607	3.989456
215.153510	5425.470486	7.659456	-0.043641	3.992308
215.323379	5433.546436	7.664461	-0.043678	3.995163
215.593495	5441.536136	7.669466	-0.043734	3.997986
215.908566	5449.549096	7.674470	-0.043798	4.000816
215.957855	5457.546828	7.679475	-0.043812	4.003634
216.174018	5465.547311	7.684480	-0.043858	4.006455
216.448576	5473.585591	7.689485	-0.043914	4.009287
216.388228	5481.642516	7.694490	-0.043908	4.012118
216.646567	5489.666381	7.699494	-0.043962	4.014941
216.941559	5497.697094	7.704499	-0.044022	4.017765
217.020086	5505.657447	7.709504	-0.044042	4.020559
217.130246	5513.719123	7.714509	-0.044068	4.023387
217.280263	5521.733120	7.719514	-0.044101	4.026197
217.482160	5529.767533	7.724518	-0.044144	4.029013
217.602248	5537.777193	7.729523	-0.044171	4.031816
217.824385	5545.859663	7.734528	-0.044218	4.034645
218.108689	5553.875574	7.739533	-0.044276	4.037450
218.096294	5561.802197	7.744538	-0.044279	4.040217
218.315427	5569.822232	7.749542	-0.044326	4.043018
218.590758	5577.826795	7.754547	-0.044382	4.045812
218.730099	5585.837225	7.759552	-0.044413	4.048605
218.939623	5593.855765	7.764557	-0.044458	4.051400
219.281208	5601.890722	7.769562	-0.044527	4.054200
219.394776	5609.921754	7.774566	-0.044553	4.056993
219.431998	5617.894031	7.779571	-0.044565	4.059763
219.634220	5625.925431	7.784576	-0.044608	4.062554
219.875733	5633.966281	7.789581	-0.044659	4.065347
220.054409	5641.958512	7.794586	-0.044697	4.068121
220.283164	5649.984048	7.799590	-0.044745	4.070904
220.515998	5658.042083	7.804595	-0.044794	4.073697
220.621545	5666.059279	7.809600	-0.044819	4.076472
220.901806	5674.039960	7.814605	-0.044876	4.079235
221.047465	5682.086530	7.819610	-0.044909	4.082017
221.315557	5690.033535	7.824614	-0.044964	4.084765
221.476730	5698.108685	7.829619	-0.044999	4.087553
221.781383	5706.081598	7.834624	-0.045061	4.090306
222.238033	5714.175711	7.839629	-0.045152	4.093101
222.011228	5722.170737	7.844634	-0.045115	4.095851
222.232092	5730.197807	7.849638	-0.045161	4.098615
222.544489	5738.196097	7.854643	-0.045225	4.101370
222.547925	5746.203202	7.859648	-0.045231	4.104121
222.639000	5754.246101	7.864653	-0.045253	4.106884
222.951995	5762.268101	7.869658	-0.045317	4.109641
223.035090	5770.300390	7.874662	-0.045337	4.112396
223.097841	5778.381681	7.879667	-0.045354	4.115166
223.554317	5786.375782	7.884672	-0.045445	4.117910
223.861201	5794.362542	7.889677	-0.045507	4.120647
223.856320	5802.343072	7.894682	-0.045512	4.123376
223.992627	5810.359509	7.899686	-0.045542	4.126117
224.329848	5818.413551	7.904691	-0.045610	4.128872
224.471203	5826.432433	7.909696	-0.045642	4.131611
224.720749	5834.468481	7.914701	-0.045694	4.134355
224.851840	5842.493028	7.919706	-0.045724	4.137092
225.191000	5850.487328	7.924710	-0.045792	4.139819
225.326478	5858.516075	7.929715	-0.045823	4.142553
225.374538	5866.483408	7.934720	-0.045837	4.145264
225.601102	5874.588634	7.939725	-0.045884	4.148022
225.796938	5882.543195	7.944730	-0.045926	4.150727
225.899989	5890.599982	7.949734	-0.045951	4.153463
226.135195	5898.661398	7.954739	-0.046000	4.156201
226.227198	5906.626143	7.959744	-0.046022	4.158902
226.447724	5914.667448	7.964749	-0.046069	4.161629
226.629006	5922.611192	7.969754	-0.046108	4.164321
226.792889	5930.705627	7.974758	-0.046144	4.167062
227.131263	5938.707452	7.979763	-0.046212	4.169771
227.150883	5946.746162	7.984768	-0.046221	4.172488
227.487080	5954.748540	7.989773	-0.046289	4.175194
227.795927	5962.758054	7.994778	-0.046352	4.177901
227.867949	5970.765577	7.999782	-0.046370	4.180602
227.994159	5978.799776	8.004787	-0.046399	4.183312
228.141576	5986.763480	8.009792	-0.046432	4.185996
228.249104	5994.805969	8.014797	-0.046457	4.188704
228.472590	6002.817642	8.019802	-0.046504	4.191401
228.736773	6010.953168	8.024806	-0.046559	4.194139
228.958682	6018.958764	8.029811	-0.046605	4.196831
229.020194	6026.892598	8.034816	-0.046622	4.199495
229.280173	6034.949328	8.039821	-0.046676	4.202201
229.499986	6042.895211	8.044826	-0.046722	4.204867
229.555769	6050.923800	8.049830	-0.046738	4.207558
229.639536	6058.898913	8.054835	-0.046759	4.210230
229.751966	6067.000542	8.059840	-0.046785	4.212942
229.891502	6075.007675	8.064845	-0.046816	4.215622
229.852790	6083.005498	8.069850	-0.046815	4.218294
230.409550	6090.993159	8.074854	-0.046923	4.220968
230.686292	6098.998783	8.079859	-0.046980	4.223643
230.815763	6107.037178	8.084864	-0.047010	4.226325
230.816858	6115.076856	8.089869	-0.047015	4.229006
231.098114	6123.095073	8.094874	-0.047073	4.231680
231.097837	6131.115035	8.099878	-0.047078	4.234350
231.338324	6139.156903	8.104883	-0.047128	4.237028
231.584618	6147.089228	8.109888	-0.047180	4.239668
231.836521	6155.222864	8.114893	-0.047232	4.242373
232.101291	6163.100975	8.119898	-0.047286	4.244992
232.341503	6171.184205	8.124902	-0.047336	4.247677
232.498978	6179.208001	8.129907	-0.047371	4.250339
232.663897	6187.246127	8.134912	-0.047407	4.253005
232.823535	6195.258399	8.139917	-0.047442	4.255661
233.012729	6203.291961	8.144922	-0.047483	4.258322
233.519618	6211.298853	8.149926	-0.047582	4.260975
233.551055	6219.337272	8.154931	-0.047594	4.263634
233.751520	6227.301775	8.159936	-0.047636	4.266267
234.015302	6235.432359	8.164941	-0.047691	4.268954
234.130898	6243.400599	8.169946	-0.047718	4.271585
234.601513	6251.464436	8.174950	-0.047811	4.274248
234.820269	6259.487579	8.179955	-0.047857	4.276894
234.705108	6267.418692	8.184960	-0.047840	4.279506
235.062649	6275.468402	8.189965	-0.047912	4.282159
235.217416	6283.435094	8.194970	-0.047946	4.284781
235.451320	6291.501739	8.199974	-0.047995	4.287435
235.493795	6299.500066	8.204979	-0.048009	4.290063
235.627396	6307.548742	8.209984	-0.048039	4.292707
236.010834	6315.587130	8.214989	-0.048116	4.295348
236.137319	6323.580360	8.219994	-0.048144	4.297971
236.401574	6331.583010	8.224998	-0.048199	4.300596
236.589763	6339.589526	8.230003	-0.048239	4.303220
236.864735	6347.599067	8.235008	-0.048296	4.305844
237.123347	6355.634977	8.240013	-0.048349	4.308475
237.055289	6363.656362	8.245018	-0.048342	4.311097
237.384948	6371.685399	8.250022	-0.048409	4.313723
237.452726	6379.700271	8.255027	-0.048427	4.316340
237.471318	6387.680907	8.260032	-0.048435	4.318945
237.946524	6395.713171	8.265037	-0.048529	4.321568
237.813992	6403.697195	8.270042	-0.048510	4.324170
237.958735	6411.751142	8.275046	-0.048542	4.326794
238.379238	6419.723777	8.280051	-0.048626	4.329393
238.476395	6427.795336	8.285056	-0.048649	4.332020
238.614347	6435.805707	8.290061	-0.048680	4.334625
238.921188	6443.827185	8.295066	-0.048743	4.337234
239.108104	6451.807926	8.300070	-0.048783	4.339827
239.304951	6459.848172	8.305075	-0.048825	4.342438
239.286483	6467.810890	8.310080	-0.048827	4.345021
239.537818	6475.919571	8.315085	-0.048879	4.347651
239.703357	6483.877791	8.320090	-0.048915	4.350231
240.028999	6491.968958	8.325094	-0.048981	4.352853
240.276158	6500.073365	8.330099	-0.049032	4.355477
240.231573	6507.997924	8.335104	-0.049029	4.358039
240.551706	6516.001631	8.340109	-0.049094	4.360628
240.743353	6523.955513	8.345114	-0.049135	4.363198
240.686225	6531.945710	8.350118	-0.049130	4.365777
240.999801	6539.981483	8.355123	-0.049193	4.368372
241.106576	6547.999638	8.360128	-0.049219	4.370958
241.318289	6556.074078	8.365133	-0.049263	4.373561
241.531429	6564.092306	8.370138	-0.049308	4.376144
241.642736	6572.095742	8.375142	-0.049335	4.378721
241.745230	6580.102151	8.380147	-0.049359	4.381297
241.951719	6588.074688	8.385152	-0.049403	4.383861
242.220898	6596.115112	8.390157	-0.049458	4.386446
242.373152	6604.126296	8.395162	-0.049492	4.389019
242.583315	6612.134515	8.400166	-0.049536	4.391590
242.637366	6620.223979	8.405171	-0.049552	4.394184
242.719600	6628.202848	8.410176	-0.049572	4.396742
242.817669	6636.208583	8.415181	-0.049596	4.399307
243.064698	6644.222635	8.420186	-0.049647	4.401874
243.310849	6652.203419	8.425190	-0.049698	4.404429
243.715543	6660.276452	8.430195	-0.049779	4.407012
243.657941	6668.244838	8.435200	-0.049774	4.409559
243.827354	6676.353394	8.440205	-0.049811	4.412149
243.776690	6684.345662	8.445210	-0.049806	4.414700
243.923564	6692.404389	8.450214	-0.049839	4.417272
244.239525	6700.395028	8.455219	-0.049903	4.419821
244.376044	6708.373250	8.460224	-0.049934	4.422364
244.917340	6716.392877	8.465229	-0.050040	4.424920
244.909025	6724.441291	8.470234	-0.050044	4.427482
245.007403	6732.403646	8.475238	-0.050067	4.430015
245.371460	6740.485087	8.480243	-0.050141	4.432586
245.507255	6748.528050	8.485248	-0.050171	4.435142
245.537724	6756.603575	8.490253	-0.050182	4.437706
245.645541	6764.503753	8.495258	-0.050208	4.440214
246.128521	6772.537851	8.500262	-0.050303	4.442764
246.378469	6780.511539	8.505267	-0.050355	4.445292
246.329430	6788.511088	8.510272	-0.050351	4.447826
246.541992	6796.544750	8.515277	-0.050396	4.450371
246.743652	6804.587173	8.520282	-0.050439	4.452917
246.771522	6812.649038	8.525286	-0.050449	4.455466
247.029682	6820.671552	8.530291	-0.050503	4.458003
247.224184	6828.633188	8.535296	-0.050544	4.460519
247.358635	6836.648497	8.540301	-0.050574	4.463050
247.412468	6844.635593	8.545306	-0.050590	4.465570
247.575393	6852.651883	8.550310	-0.050625	4.468099
247.828043	6860.676857	8.555315	-0.050678	4.470629
248.134843	6868.724801	8.560320	-0.050740	4.473165
248.410999	6876.785668	8.565325	-0.050797	4.475703
248.421970	6884.735570	8.570330	-0.050804	4.478204
248.641793	6892.730740	8.575335	-0.050851	4.480719
248.779540	6900.784883	8.580339	-0.050882	4.483251
249.220514	6908.754517	8.585344	-0.050969	4.485755
249.392609	6916.830543	8.590349	-0.051006	4.488291
249.525523	6924.835889	8.595354	-0.051037	4.490803
249.674361	6932.857601	8.600359	-0.051070	4.493319
249.890962	6940.867398	8.605363	-0.051115	4.495829
249.957437	6948.872948	8.610368	-0.051133	4.498337
250.185412	6956.911720	8.615373	-0.051181	4.500854
250.529487	6964.871396	8.620378	-0.051250	4.503345
250.626823	6972.899293	8.625383	-0.051273	4.505855
250.773721	6980.936369	8.630387	-0.051306	4.508367
251.042866	6988.919184	8.635392	-0.051362	4.510861
251.188224	6997.029387	8.640397	-0.051394	4.513393
251.232495	7005.053757	8.645402	-0.051408	4.515897
251.541704	7013.019894	8.650407	-0.051470	4.518381
251.895238	7021.031370	8.655411	-0.051542	4.520878
252.020014	7029.011632	8.660416	-0.051570	4.523364
252.245666	7037.032903	8.665421	-0.051617	4.525862
252.482026	7045.026524	8.670426	-0.051667	4.528349
252.677371	7053.031882	8.675431	-0.051709	4.530838
252.751214	7061.102620	8.680435	-0.051728	4.533347
252.979460	7069.086644	8.685440	-0.051775	4.535827
253.043886	7077.138250	8.690445	-0.051793	4.538326
252.902636	7085.120735	8.695450	-0.051772	4.540802
253.463419	7093.111674	8.700455	-0.051881	4.543281
253.670101	7101.133793	8.705459	-0.051925	4.545767
253.690414	7109.184282	8.710464	-0.051934	4.548261
253.962652	7117.219144	8.715469	-0.051990	4.550749
254.156280	7125.265847	8.720474	-0.052032	4.553238
254.377748	7133.314931	8.725479	-0.052078	4.555728
254.412297	7141.280145	8.730483	-0.052090	4.558189
254.731873	7149.203404	8.735488	-0.052155	4.560637
254.881751	7157.309523	8.740493	-0.052188	4.563139
254.978607	7165.272515	8.745498	-0.052212	4.565596
255.410409	7173.340383	8.750503	-0.052297	4.568085
255.606414	7181.351486	8.755507	-0.052339	4.570554
255.631184	7189.356159	8.760512	-0.052349	4.573020
255.978705	7197.416392	8.765517	-0.052419	4.575501
255.969106	7205.390299	8.770522	-0.052423	4.577955
256.050287	7213.407983	8.775527	-0.052443	4.580421
256.227369	7221.451268	8.780531	-0.052481	4.582893
256.318121	7229.421785	8.785536	-0.052504	4.585342
256.635451	7237.477837	8.790541	-0.052568	4.587815
256.837603	7245.484482	8.795546	-0.052611	4.590272
257.124186	7253.530106	8.800551	-0.052670	4.592740
257.385921	7261.556746	8.805555	-0.052724	4.595200
257.363885	7269.558185	8.810560	-0.052725	4.597652
257.440775	7277.544556	8.815565	-0.052745	4.600097
257.617796	7285.590374	8.820570	-0.052783	4.602559
257.774940	7293.529279	8.825575	-0.052817	4.604988
258.079117	7301.615596	8.830579	-0.052879	4.607460
258.162663	7309.564061	8.835584	-0.052900	4.609888
258.474899	7317.623420	8.840589	-0.052964	4.612349
258.554380	7325.647971	8.845594	-0.052984	4.614799
258.685883	7333.682034	8.850599	-0.053014	4.617249
258.855249	7341.639584	8.855603	-0.053050	4.619676
258.918592	7349.708765	8.860608	-0.053068	4.622134
259.013495	7357.668539	8.865613	-0.053091	4.624559
259.329753	7365.709013	8.870618	-0.053155	4.627006
259.503043	7373.727823	8.875623	-0.053192	4.629446
259.606061	7381.786675	8.880627	-0.053217	4.631896
259.696412	7389.781989	8.885632	-0.053239	4.634326
260.169789	7397.782818	8.890637	-0.053332	4.636756
260.225999	7405.756735	8.895642	-0.053348	4.639176
260.196300	7413.799363	8.900647	-0.053348	4.641617
260.510817	7421.790938	8.905651	-0.053412	4.644040
260.753117	7429.786519	8.910656	-0.053462	4.646464
261.015934	7437.818421	8.915661	-0.053517	4.648897
261.118789	7445.878671	8.920666	-0.053541	4.651337
261.172202	7453.940906	8.925671	-0.053556	4.653777
261.280244	7461.948821	8.930675	-0.053582	4.656199
261.420730	7469.886749	8.935680	-0.053613	4.658598
261.771431	7477.921926	8.940685	-0.053684	4.661026
262.081667	7485.931228	8.945690	-0.053747	4.663444
262.110496	7493.958733	8.950695	-0.053758	4.665867
262.176706	7501.994791	8.955699	-0.053775	4.668291
262.241158	7509.971873	8.960704	-0.053793	4.670697
262.546020	7518.094499	8.965709	-0.053855	4.673144
262.786871	7526.129862	8.970714	-0.053905	4.675564
262.930597	7534.107640	8.975719	-0.053937	4.677965
263.055056	7542.051049	8.980723	-0.053966	4.680355
263.193069	7550.058895	8.985728	-0.053997	4.682763
263.381612	7558.039085	8.990733	-0.054037	4.685161
263.638396	7566.102953	8.995738	-0.054090	4.687583
263.618105	7574.040020	9.000743	-0.054092	4.689967
263.878380	7582.132122	9.005747	-0.054145	4.692395
263.956147	7590.107333	9.010752	-0.054165	4.694787
264.293927	7598.188788	9.015757	-0.054233	4.697209
264.394576	7606.123524	9.020762	-0.054257	4.699586
264.605994	7614.199873	9.025767	-0.054302	4.702005
264.576590	7622.210534	9.030771	-0.054302	4.704403
264.741843	7630.190505	9.035776	-0.054338	4.706790
265.033837	7638.232160	9.040781	-0.054398	4.709194
265.153144	7646.217908	9.045786	-0.054425	4.711580
265.312503	7654.242642	9.050791	-0.054460	4.713977
265.424648	7662.290938	9.055795	-0.054487	4.716380
265.671874	7670.278817	9.060800	-0.054538	4.718763
265.849205	7678.303627	9.065805	-0.054576	4.721156
266.038319	7686.300236	9.070810	-0.054617	4.723539
266.221563	7694.327103	9.075815	-0.054656	4.725930
266.415840	7702.405421	9.080819	-0.054698	4.728335
266.318293	7710.423876	9.085824	-0.054685	4.730722
266.647699	7718.428040	9.090829	-0.054752	4.733103
266.769883	7726.422456	9.095834	-0.054780	4.735479
266.904319	7734.442099	9.100839	-0.054810	4.737862
267.199782	7742.450919	9.105843	-0.054870	4.740240
267.167819	7750.444182	9.110848	-0.054870	4.742614
267.271844	7758.439944	9.115853	-0.054894	4.744986
267.339258	7766.468783	9.120858	-0.054912	4.747367
267.848031	7774.491434	9.125863	-0.055012	4.749744
268.000984	7782.527467	9.130867	-0.055046	4.752124
268.157081	7790.563419	9.135872	-0.055081	4.754504
268.265681	7798.636599	9.140877	-0.055106	4.756893
268.402119	7806.555934	9.145882	-0.055137	4.759235
268.594803	7814.587709	9.150887	-0.055178	4.761610
268.787950	7822.554904	9.155891	-0.055219	4.763964
268.898556	7830.578883	9.160896	-0.055245	4.766333
269.306826	7838.625924	9.165901	-0.055327	4.768708
269.533934	7846.642798	9.170906	-0.055374	4.771073
269.508124	7854.674890	9.175911	-0.055375	4.773442
269.658844	7862.690269	9.180915	-0.055408	4.775804
269.591024	7870.658732	9.185920	-0.055401	4.778153
270.072093	7878.684992	9.190925	-0.055496	4.780515
270.056674	7886.712049	9.195930	-0.055498	4.782878
270.119797	7894.649839	9.200935	-0.055515	4.785213
270.543214	7902.770284	9.205939	-0.055599	4.787599
270.787287	7910.723177	9.210944	-0.055650	4.789936
270.837419	7918.854440	9.215949	-0.055665	4.792324
270.837430	7926.814562	9.220954	-0.055670	4.794662
271.133527	7934.836662	9.225959	-0.055731	4.797015
271.433052	7942.822430	9.230963	-0.055792	4.799356
271.508705	7950.818022	9.235968	-0.055811	4.801700
271.608160	7958.824358	9.240973	-0.055835	4.804046
271.877536	7966.846121	9.245978	-0.055890	4.806394
271.971517	7974.821921	9.250983	-0.055913	4.808729
272.231221	7982.889942	9.255987	-0.055967	4.811088
272.343065	7990.380723	9.260992	-0.055993	4.813279
272.646734	7995.071628	9.265997	-0.056052	4.814649

272.650705	7997.708675	9.271002	-0.056055	4.815419
272.704439	7999.061947	9.276007	-0.056066	4.815815
272.774846	7999.499063	9.281011	-0.056079	4.815942
272.861168	8000.494126	9.286016	-0.056096	4.816232
272.972777	8000.596578	9.291021	-0.056117	4.816262
273.233815	8000.573542	9.296026	-0.056166	4.816254
273.183065	8000.581178	9.301031	-0.056156	4.816256
273.163257	8000.588307	9.306035	-0.056153	4.816258
273.518906	8000.562712	9.311040	-0.056219	4.816249
273.478028	8000.586552	9.316045	-0.056212	4.816256
273.308019	8000.557841	9.321050	-0.056180	4.816249
273.355379	8000.528796	9.326055	-0.056189	4.816240
273.690958	8000.511384	9.331059	-0.056252	4.816233
273.665514	8000.586784	9.336064	-0.056247	4.816255
273.687294	8000.575436	9.341069	-0.056251	4.816252
273.570667	8000.609655	9.346074	-0.056230	4.816262
273.732281	8000.512171	9.351079	-0.056260	4.816233
273.853931	8000.620150	9.356083	-0.056282	4.816264
273.809602	8000.567008	9.361088	-0.056274	4.816249
273.829751	8000.468028	9.366093	-0.056278	4.816220
273.925893	8000.573408	9.371098	-0.056296	4.816250
274.038958	8000.551964	9.376103	-0.056317	4.816243
274.100842	8000.602239	9.381107	-0.056329	4.816257
273.938651	8000.585420	9.386112	-0.056299	4.816253
274.080333	8000.479028	9.391117	-0.056325	4.816222
274.096096	8000.600045	9.396122	-0.056328	4.816257
274.037603	8000.514596	9.401127	-0.056317	4.816232
274.201774	8000.629757	9.406131	-0.056348	4.816265
274.352172	8000.503224	9.411136	-0.056376	4.816227
274.407694	8000.514923	9.416141	-0.056387	4.816230
274.351753	8000.605796	9.421146	-0.056376	4.816257
274.264810	8000.542265	9.426151	-0.056360	4.816239
274.429583	8000.530305	9.431155	-0.056391	4.816235
274.248062	8000.512068	9.436160	-0.056357	4.816230
274.350926	8000.620776	9.441165	-0.056377	4.816261
274.620205	8000.496398	9.446170	-0.056427	4.816224
274.384727	8000.572264	9.451175	-0.056383	4.816247
274.390149	8000.541390	9.456179	-0.056384	4.816238
274.314729	8000.583834	9.461184	-0.056370	4.816251
274.513606	8000.558604	9.466189	-0.056407	4.816242
274.559166	8000.519911	9.471194	-0.056416	4.816231
274.549507	8000.546454	9.476199	-0.056414	4.816239
274.507368	8000.526469	9.481203	-0.056407	4.816233
274.630189	8000.584260	9.486208	-0.056430	4.816249
274.800665	8000.529669	9.491213	-0.056461	4.816232
274.824430	8000.610237	9.496218	-0.056466	4.816256
274.640506	8000.507555	9.501223	-0.056432	4.816227
274.475767	8000.612481	9.506227	-0.056401	4.816258
274.595646	8000.507829	9.511232	-0.056424	4.816227
274.814104	8000.479748	9.516237	-0.056464	4.816218
274.754638	8000.612224	9.521242	-0.056453	4.816257
274.572409	8000.474317	9.526247	-0.056420	4.816217
274.849211	8000.603274	9.531251	-0.056471	4.816254
274.616633	8000.569153	9.536256	-0.056428	4.816245
274.744293	8000.531948	9.541261	-0.056452	4.816233
274.681054	8000.469915	9.546266	-0.056440	4.816216
274.786017	8000.600030	9.551271	-0.056460	4.816253
274.845263	8000.558380	9.556275	-0.056471	4.816241
274.817700	8000.617718	9.561280	-0.056466	4.816258
274.923511	8000.378198	9.566285	-0.056486	4.816187
275.054125	8000.612409	9.571290	-0.056510	4.816255
274.949106	8000.556028	9.576295	-0.056491	4.816239
275.087566	8000.494446	9.581299	-0.056517	4.816221
274.840289	8000.595739	9.586304	-0.056471	4.816251
274.950909	8000.471689	9.591309	-0.056491	4.816215
274.995047	8000.554762	9.596314	-0.056500	4.816239
275.031951	8000.578945	9.601319	-0.056507	4.816246
274.952938	8000.585000	9.606323	-0.056492	4.816248
275.023668	8000.488003	9.611328	-0.056505	4.816219
275.352426	8000.600811	9.616333	-0.056567	4.816250
275.050007	8000.602815	9.621338	-0.056510	4.816252
275.030606	8000.463586	9.626343	-0.056507	4.816212
275.179116	8000.525048	9.631347	-0.056535	4.816229
275.225282	8000.589996	9.636352	-0.056543	4.816248
275.262757	8000.458208	9.641357	-0.056550	4.816209
275.163686	8000.626291	9.646362	-0.056532	4.816259
275.240438	8000.500557	9.651367	-0.056546	4.816222
275.224155	8000.533391	9.656371	-0.056543	4.816231
275.106030	8000.598565	9.661376	-0.056522	4.816251
275.472319	8000.497313	9.666381	-0.056590	4.816219
275.331700	8000.619771	9.671386	-0.056564	4.816256
275.199028	8000.582118	9.676391	-0.056539	4.816246
275.423317	8000.557350	9.681395	-0.056581	4.816237
275.282393	8000.512069	9.686400	-0.056555	4.816225
275.336272	8000.521602	9.691405	-0.056565	4.816227
275.361088	8000.631036	9.696410	-0.056570	4.816259
275.404645	8000.490810	9.701415	-0.056578	4.816218
275.381473	8000.538476	9.706419	-0.056574	4.816232
275.168292	8000.568808	9.711424	-0.056534	4.816242
275.375593	8000.591807	9.716429	-0.056573	4.816247
275.375563	8000.509552	9.721434	-0.056573	4.816223
275.311576	8000.541520	9.726439	-0.056561	4.816233
275.240961	8000.580847	9.731443	-0.056548	4.816245
275.421763	8000.600162	9.736448	-0.056582	4.816250
275.437129	8000.497886	9.741453	-0.056585	4.816220
275.386184	8000.590988	9.746458	-0.056575	4.816247
275.449490	8000.571847	9.751463	-0.056587	4.816241
275.589926	8000.529532	9.756467	-0.056614	4.816228
275.399623	8000.580577	9.761472	-0.056578	4.816244
275.618952	8000.580291	9.766477	-0.056619	4.816243
275.670821	8000.460515	9.771482	-0.056629	4.816207
275.421171	8000.461339	9.776487	-0.056582	4.816209
275.460339	8000.572101	9.781491	-0.056590	4.816241
275.543666	8000.543708	9.786496	-0.056606	4.816232
275.542529	8000.620620	9.791501	-0.056605	4.816255
275.412952	8000.529604	9.796506	-0.056581	4.816229
275.669328	8000.566315	9.801511	-0.056629	4.816238
275.659927	8000.489231	9.806515	-0.056628	4.816216
275.556158	8000.524752	9.811520	-0.056608	4.816227
275.494420	8000.542872	9.816525	-0.056597	4.816232
275.696759	8000.606381	9.821530	-0.056635	4.816250
275.796958	8000.555857	9.826535	-0.056653	4.816235
275.778927	8000.481822	9.831539	-0.056650	4.816213
275.843895	8000.601600	9.836544	-0.056662	4.816248
275.947326	8000.510536	9.841549	-0.056682	4.816221
275.634999	8000.604240	9.846554	-0.056624	4.816250
275.856341	8000.537751	9.851559	-0.056665	4.816229
275.871790	8000.576503	9.856563	-0.056668	4.816240
275.731978	8000.542993	9.861568	-0.056642	4.816231
275.848957	8000.481022	9.866573	-0.056664	4.816212
275.739545	8000.616868	9.871578	-0.056644	4.816253
275.643253	8000.462353	9.876583	-0.056626	4.816208
275.660839	8000.624007	9.881587	-0.056629	4.816255
275.971352	8000.522811	9.886592	-0.056687	4.816224
276.048793	8000.566960	9.891597	-0.056702	4.816237
275.911589	8000.521746	9.896602	-0.056676	4.816224
275.995868	8000.588455	9.901607	-0.056692	4.816243
276.034620	8000.533612	9.906611	-0.056699	4.816227
275.904786	8000.553702	9.911616	-0.056675	4.816233
275.981067	8000.562574	9.916621	-0.056690	4.816236
276.000710	8000.518068	9.921626	-0.056693	4.816222
276.061472	8000.567257	9.926631	-0.056705	4.816237
275.829526	8000.584427	9.931635	-0.056662	4.816243
275.840574	8000.593184	9.936640	-0.056664	4.816245
275.980609	8000.470733	9.941645	-0.056690	4.816209
275.857178	8000.570000	9.946650	-0.056667	4.816238
275.879640	8000.528750	9.951655	-0.056671	4.816226
276.122191	8000.615426	9.956659	-0.056717	4.816250
275.862870	8000.587226	9.961664	-0.056668	4.816243
276.274816	8000.442998	9.966669	-0.056745	4.816199
275.971474	8000.619130	9.971674	-0.056689	4.816252
276.014302	8000.582523	9.976679	-0.056697	4.816241
276.148874	8000.539033	9.981683	-0.056722	4.816228
276.164528	8000.519028	9.986688	-0.056725	4.816222
276.039896	8000.557375	9.991693	-0.056702	4.816234
275.928264	8000.533992	9.996698	-0.056681	4.816227
276.013823	8000.564400	10.001703	-0.056697	4.816236
276.145835	8000.541163	10.006707	-0.056722	4.816228
276.016547	8000.637119	10.011712	-0.056698	4.816257
276.036000	8000.534916	10.016717	-0.056702	4.816227
276.263091	8000.555071	10.021722	-0.056744	4.816232
276.311540	8000.566644	10.026727	-0.056753	4.816235
276.169673	8000.454036	10.031731	-0.056727	4.816203
276.075055	8000.592287	10.036736	-0.056709	4.816244
276.130390	8000.560181	10.041741	-0.056720	4.816234
276.317871	8000.474915	10.046746	-0.056755	4.816208
275.990248	8000.402742	10.051751	-0.056694	4.816189
276.098022	8000.657914	10.056755	-0.056714	4.816263
276.116767	8000.623007	10.061760	-0.056718	4.816252
276.247870	8000.425606	10.066765	-0.056742	4.816194
276.317284	8000.532645	10.071770	-0.056755	4.816225
276.252252	8000.585963	10.076775	-0.056743	4.816241
276.103291	8000.554424	10.081779	-0.056716	4.816232
275.943760	8000.593206	10.086784	-0.056686	4.816245
275.956787	8000.537896	10.091789	-0.056688	4.816228
276.075148	8000.508001	10.096794	-0.056711	4.816219
275.971469	8000.517882	10.101799	-0.056691	4.816222
276.171203	8000.547157	10.106803	-0.056729	4.816230
276.060204	8000.597503	10.111808	-0.056708	4.816245
275.967498	8000.601173	10.116813	-0.056691	4.816247
276.052712	8000.535420	10.121818	-0.056707	4.816227
276.362555	8000.565624	10.126823	-0.056765	4.816234
276.251567	8000.485627	10.131827	-0.056744	4.816212
276.136743	8000.520947	10.136832	-0.056723	4.816222
276.346518	8000.600619	10.141837	-0.056762	4.816245
276.333173	8000.497820	10.146842	-0.056760	4.816215
276.212342	8000.512732	10.151847	-0.056737	4.816220
276.153748	8000.620655	10.156851	-0.056726	4.816251
276.049418	8000.494838	10.161856	-0.056707	4.816215
276.081763	8000.571290	10.166861	-0.056713	4.816237
276.132521	8000.581836	10.171866	-0.056723	4.816240
276.140597	8000.563830	10.176871	-0.056724	4.816235
276.083889	8000.544648	10.181875	-0.056714	4.816230
275.945143	8000.505815	10.186880	-0.056688	4.816219
276.162782	8000.614475	10.191885	-0.056729	4.816250
276.136110	8000.599043	10.196890	-0.056724	4.816245
276.129276	8000.499569	10.201895	-0.056723	4.816216
276.456225	8000.545040	10.206899	-0.056784	4.816228
276.457580	8000.598494	10.211904	-0.056784	4.816243
276.503477	8000.605747	10.216909	-0.056793	4.816245
276.363392	8000.538043	10.221914	-0.056767	4.816226
276.228707	8000.491805	10.226919	-0.056742	4.816213
276.391325	8000.564210	10.231923	-0.056772	4.816234
276.167429	8000.556953	10.236928	-0.056731	4.816233
276.317349	8000.529767	10.241933	-0.056759	4.816224
276.311200	8000.414279	10.246938	-0.056757	4.816190
276.277279	8000.448930	10.251943	-0.056751	4.816201
276.395142	8000.561122	10.256947	-0.056773	4.816233
276.336966	8000.624180	10.261952	-0.056763	4.816251
276.408449	8000.417150	10.266957	-0.056776	4.816191
276.362137	8000.593672	10.271962	-0.056767	4.816242
276.323389	8000.548106	10.276967	-0.056760	4.816229
276.577481	8000.421313	10.281971	-0.056808	4.816191
276.398206	8000.637092	10.286976	-0.056775	4.816255
276.586564	8000.451412	10.291981	-0.056810	4.816200
276.626787	8000.575017	10.296986	-0.056817	4.816236
276.576676	8000.512151	10.301991	-0.056808	4.816217
276.387821	8000.576043	10.306995	-0.056773	4.816237
276.604329	8000.588528	10.312000	-0.056813	4.816240
276.688334	8000.463990	10.317005	-0.056829	4.816203
276.529234	8000.641673	10.322010	-0.056800	4.816256
276.590931	8000.528483	10.327015	-0.056811	4.816222
276.614852	8000.571663	10.332019	-0.056816	4.816235
276.417112	8000.643941	10.337024	-0.056779	4.816257
276.552567	8000.520337	10.342029	-0.056804	4.816220
276.566953	8000.570822	10.347034	-0.056807	4.816235
276.400750	8000.547517	10.352039	-0.056776	4.816229
276.431026	8000.556623	10.357043	-0.056782	4.816231
276.564685	8000.474654	10.362048	-0.056807	4.816207
276.545887	8000.514922	10.367053	-0.056804	4.816218
276.586065	8000.554123	10.372058	-0.056811	4.816230
276.591825	8000.561715	10.377063	-0.056812	4.816232
276.627321	8000.516428	10.382067	-0.056819	4.816218
276.660770	8000.621748	10.387072	-0.056825	4.816249
276.723260	8000.469041	10.392077	-0.056837	4.816204
276.829754	8000.543635	10.397082	-0.056857	4.816225
276.651725	8000.568192	10.402087	-0.056824	4.816233
276.633649	8000.544369	10.407091	-0.056821	4.816227
276.646706	8000.547821	10.412096	-0.056823	4.816227
276.736905	8000.465063	10.417101	-0.056840	4.816203
276.657065	8000.505292	10.422106	-0.056825	4.816215
276.709316	8000.568217	10.427111	-0.056835	4.816233
276.798908	8000.583741	10.432115	-0.056852	4.816237
276.630999	8000.539036	10.437120	-0.056821	4.816225
276.835045	8000.519244	10.442125	-0.056859	4.816218
276.922108	8000.598827	10.447130	-0.056875	4.816241
276.900854	8000.554646	10.452135	-0.056871	4.816228
276.793324	8000.527062	10.457139	-0.056851	4.816221
276.718552	8000.624009	10.462144	-0.056838	4.816249
276.849202	8000.555874	10.467149	-0.056862	4.816229
276.890682	8000.544884	10.472154	-0.056870	4.816225
276.757850	8000.538210	10.477159	-0.056845	4.816224
277.038570	8000.543313	10.482163	-0.056898	4.816224
276.778224	8000.553556	10.487168	-0.056849	4.816228
276.758748	8000.517955	10.492173	-0.056846	4.816218
276.834786	8000.543918	10.497178	-0.056860	4.816225
276.762524	8000.529795	10.502183	-0.056847	4.816222
276.826923	8000.565162	10.507187	-0.056859	4.816232
276.892246	8000.605888	10.512192	-0.056871	4.816243
276.914453	8000.525102	10.517197	-0.056875	4.816219
276.862198	8000.558352	10.522202	-0.056865	4.816229
276.732199	8000.640407	10.527207	-0.056841	4.816254
276.890131	8000.554605	10.532211	-0.056871	4.816228
276.950140	8000.504420	10.537216	-0.056882	4.816213
276.708252	8000.645343	10.542221	-0.056837	4.816256
276.853927	8000.431110	10.547226	-0.056864	4.816192
276.995708	8000.633485	10.552231	-0.056891	4.816251
276.911167	8000.459946	10.557235	-0.056875	4.816200
276.737565	8000.619203	10.562240	-0.056843	4.816248
276.920987	8000.541342	10.567245	-0.056877	4.816224
276.854282	8000.518773	10.572250	-0.056865	4.816218
276.834328	8000.522694	10.577255	-0.056861	4.816219
276.936592	8000.555543	10.582259	-0.056881	4.816228
276.836761	8000.574041	10.587264	-0.056862	4.816234
276.820260	8000.392123	10.592269	-0.056859	4.816181
276.932827	8000.378149	10.597274	-0.056880	4.816176
276.731943	8000.442891	10.602279	-0.056843	4.816196
276.741666	8000.388589	10.607283	-0.056845	4.816180
276.790332	8000.487774	10.612288	-0.056854	4.816209
277.000669	8000.624084	10.617293	-0.056893	4.816248
276.916476	8000.560597	10.622298	-0.056878	4.816230
276.849214	8000.510239	10.627303	-0.056865	4.816215
277.110354	8000.652814	10.632307	-0.056914	4.816256
277.006903	8000.522736	10.637312	-0.056895	4.816218
276.853484	8000.507140	10.642317	-0.056866	4.816214
276.849881	8000.652388	10.647322	-0.056866	4.816257
276.842736	8000.484528	10.652327	-0.056864	4.816208
277.154723	8000.373742	10.657331	-0.056922	4.816174
276.944922	8000.553711	10.662336	-0.056884	4.816227
277.077226	8000.574285	10.667341	-0.056908	4.816233
276.985624	8000.569427	10.672346	-0.056891	4.816232
276.870115	8000.411353	10.677351	-0.056870	4.816186
277.067933	8000.523929	10.682355	-0.056907	4.816218
276.986548	8000.631440	10.687360	-0.056892	4.816250
276.992910	8000.564255	10.692365	-0.056893	4.816230
276.992412	8000.518314	10.697370	-0.056893	4.816217
276.860620	8000.528753	10.702375	-0.056869	4.816221
277.128373	8000.541100	10.707379	-0.056919	4.816223
277.087158	8000.518994	10.712384	-0.056911	4.816217
277.101487	8000.361139	10.717389	-0.056914	4.816170
277.081772	8000.550967	10.722394	-0.056910	4.816226
277.105600	8000.620857	10.727399	-0.056915	4.816246
277.128626	8000.425764	10.732403	-0.056919	4.816189
277.318227	8000.633283	10.737408	-0.056955	4.816249
277.085095	8000.532903	10.742413	-0.056911	4.816221
277.085496	8000.559630	10.747418	-0.056911	4.816228
277.141362	8000.488002	10.752423	-0.056922	4.816207
277.119233	8000.417095	10.757427	-0.056918	4.816187
277.187244	8000.625611	10.762432	-0.056931	4.816247
277.217631	8000.438131	10.767437	-0.056936	4.816192
277.321355	8000.510538	10.772442	-0.056956	4.816213
277.017597	8000.625766	10.777447	-0.056899	4.816248
277.224124	8000.451098	10.782451	-0.056938	4.816196
277.135127	8000.637534	10.787456	-0.056922	4.816251
277.115404	8000.530344	10.792461	-0.056918	4.816220
277.219217	8000.405096	10.797466	-0.056937	4.816182
277.012761	8000.422728	10.802471	-0.056899	4.816189
277.031151	8000.414524	10.807475	-0.056902	4.816186
276.883096	8000.647965	10.812480	-0.056875	4.816255
277.054807	8000.390399	10.817485	-0.056907	4.816179
277.161850	8000.532312	10.822490	-0.056927	4.816220
276.997335	8000.603057	10.827495	-0.056897	4.816242
277.136698	8000.560722	10.832499	-0.056923	4.816228
277.034516	8000.532167	10.837504	-0.056904	4.816221
276.988140	8000.539882	10.842509	-0.056895	4.816223
277.082280	8000.551216	10.847514	-0.056913	4.816226
276.968934	8000.568400	10.852519	-0.056892	4.816232
277.303218	8000.449472	10.857523	-0.056954	4.816195
277.190060	8000.630127	10.862528	-0.056933	4.816248
277.301890	8000.572335	10.867533	-0.056954	4.816231
277.312787	8000.526600	10.872538	-0.056956	4.816217
277.015118	8000.563944	10.877543	-0.056901	4.816230
277.034223	8000.531180	10.882547	-0.056905	4.816220
277.121900	8000.577654	10.887552	-0.056921	4.816233
277.332906	8000.515251	10.892557	-0.056960	4.816214
277.251820	8000.537294	10.897562	-0.056945	4.816221
277.055966	8000.587170	10.902567	-0.056909	4.816237
277.150525	8000.531201	10.907571	-0.056927	4.816220
277.106844	8000.554992	10.912576	-0.056919	4.816227
277.205182	8000.571744	10.917581	-0.056937	4.816231
277.115680	8000.633166	10.922586	-0.056921	4.816250
276.992656	8000.548674	10.927591	-0.056898	4.816226
277.254563	8000.561985	10.932595	-0.056947	4.816228
277.250727	8000.593977	10.937600	-0.056946	4.816237
277.192533	8000.542715	10.942605	-0.056935	4.816223
277.134095	8000.411318	10.947610	-0.056924	4.816185
277.251587	8000.554490	10.952615	-0.056946	4.816226
277.193232	8000.571604	10.957619	-0.056936	4.816231
277.100305	8000.593432	10.962624	-0.056918	4.816238
277.233317	8000.584103	10.967629	-0.056943	4.816235
277.213572	8000.468365	10.972634	-0.056940	4.816201
277.386406	8000.555917	10.977639	-0.056972	4.816226
277.392229	8000.545348	10.982643	-0.056973	4.816222
277.121004	8000.609882	10.987648	-0.056923	4.816243
277.261568	8000.516285	10.992653	-0.056949	4.816215
277.091263	8000.631798	10.997658	-0.056918	4.816249
277.143436	8000.567581	11.002663	-0.056927	4.816230
277.227381	8000.482572	11.007667	-0.056943	4.816205
277.231340	8000.600180	11.012672	-0.056944	4.816239
277.274557	8000.489858	11.017677	-0.056952	4.816207
277.339498	8000.258133	11.022682	-0.056964	4.816139
277.091989	8000.567763	11.027687	-0.056918	4.816231
277.245909	8000.415646	11.032691	-0.056947	4.816185
277.227654	8000.540329	11.037696	-0.056944	4.816222
277.164804	8000.494325	11.042701	-0.056932	4.816209
277.216756	8000.642719	11.047706	-0.056942	4.816252
277.332724	8000.517691	11.052711	-0.056963	4.816215
277.412737	8000.553342	11.057715	-0.056979	4.816225
277.270477	8000.448202	11.062720	-0.056952	4.816195
277.203152	8000.602979	11.067725	-0.056940	4.816240
277.174339	8000.547976	11.072730	-0.056934	4.816224
277.164209	8000.604428	11.077735	-0.056933	4.816241
277.133555	8000.536571	11.082739	-0.056927	4.816221
277.121557	8000.632520	11.087744	-0.056925	4.816249
277.158396	8000.517809	11.092749	-0.056932	4.816216
277.048913	8000.606647	11.097754	-0.056912	4.816242
277.334468	8000.607566	11.102759	-0.056965	4.816241
277.485446	8000.517363	11.107763	-0.056993	4.816214
277.338356	8000.609793	11.112768	-0.056966	4.816242
277.438015	8000.481264	11.117773	-0.056984	4.816203
277.285727	8000.531930	11.122778	-0.056956	4.816219
277.267183	8000.641651	11.127783	-0.056953	4.816251
277.400775	8000.548995	11.132787	-0.056978	4.816223
277.294764	8000.596228	11.137792	-0.056958	4.816238
277.343037	8000.471040	11.142797	-0.056967	4.816201
277.291931	8000.527817	11.147802	-0.056958	4.816218
277.246255	8000.560119	11.152807	-0.056949	4.816227
277.370671	8000.626492	11.157811	-0.056973	4.816246
277.285827	8000.509572	11.162816	-0.056957	4.816212
277.256116	8000.531479	11.167821	-0.056951	4.816219
277.217233	8000.464541	11.172826	-0.056944	4.816200
277.256128	8000.578509	11.177831	-0.056952	4.816233
277.219340	8000.511609	11.182835	-0.056945	4.816213
277.277609	8000.621655	11.187840	-0.056956	4.816245
277.249346	8000.484394	11.192845	-0.056951	4.816205
277.319710	8000.529485	11.197850	-0.056964	4.816218
277.176811	8000.599554	11.202855	-0.056937	4.816239
277.227404	8000.515008	11.207859	-0.056947	4.816214
277.225447	8000.511777	11.212864	-0.056947	4.816213
277.166111	8000.561994	11.217869	-0.056936	4.816228
277.301256	8000.534540	11.222874	-0.056961	4.816220
277.442614	8000.618316	11.227879	-0.056987	4.816243
277.349154	8000.425382	11.232883	-0.056970	4.816187
277.261497	8000.573379	11.237888	-0.056954	4.816231
277.198864	8000.435495	11.242893	-0.056942	4.816191
277.283663	8000.570595	11.247898	-0.056958	4.816230
277.134121	8000.502717	11.252903	-0.056930	4.816211
277.310488	8000.606359	11.257907	-0.056963	4.816241
277.228294	8000.578166	11.262912	-0.056948	4.816233
277.356605	8000.482210	11.267917	-0.056972	4.816204
277.295874	8000.534539	11.272922	-0.056961	4.816220
277.611633	8000.476174	11.277927	-0.057020	4.816201
277.540472	8000.574255	11.282931	-0.057007	4.816230
277.455449	8000.673154	11.287936	-0.056991	4.816259
277.562084	8000.475303	11.292941	-0.057011	4.816201
277.611772	8000.589468	11.297946	-0.057020	4.816234
277.413257	8000.501469	11.302951	-0.056983	4.816209
277.428421	8000.509232	11.307955	-0.056986	4.816212
277.324993	8000.634507	11.312960	-0.056967	4.816249
277.395121	8000.492621	11.317965	-0.056980	4.816207
277.340164	8000.541849	11.322970	-0.056970	4.816222
277.413661	8000.560287	11.327975	-0.056984	4.816227
277.366843	8000.462221	11.332979	-0.056975	4.816198
277.194848	8000.649287	11.337984	-0.056943	4.816254
277.545475	8000.524245	11.342989	-0.057009	4.816215
277.576607	8000.460714	11.347994	-0.057015	4.816197
277.299507	8000.654421	11.352999	-0.056963	4.816255
277.511396	8000.429634	11.358003	-0.057003	4.816188
277.308623	8000.637511	11.363008	-0.056965	4.816250
277.213480	8000.513994	11.368013	-0.056947	4.816214
277.279949	8000.526962	11.373018	-0.056960	4.816217
277.430291	8000.566027	11.378023	-0.056988	4.816228
277.604944	8000.523264	11.383027	-0.057021	4.816215
277.541418	8000.603321	11.388032	-0.057009	4.816238
277.518080	8000.578333	11.393037	-0.057005	4.816231
277.593174	8000.522011	11.398042	-0.057019	4.816214
277.572955	8000.639181	11.403047	-0.057015	4.816249
277.639400	8000.434190	11.408051	-0.057028	4.816188
277.552648	8000.630284	11.413056	-0.057012	4.816246
277.389922	8000.452118	11.418061	-0.056981	4.816195
277.374017	8000.519149	11.423066	-0.056978	4.816215
277.488347	8000.630214	11.428071	-0.057000	4.816246
277.469129	8000.341401	11.433075	-0.056996	4.816162
277.499113	8000.575939	11.438080	-0.057002	4.816231
277.631110	8000.489665	11.443085	-0.057027	4.816205
277.696778	8000.604120	11.448090	-0.057039	4.816238
277.519063	8000.486582	11.453095	-0.057006	4.816204
277.555978	8000.619746	11.458099	-0.057013	4.816243
277.551076	8000.582272	11.463104	-0.057012	4.816232
277.441469	8000.519392	11.468109	-0.056992	4.816214
277.460256	8000.652227	11.473114	-0.056996	4.816253
277.602619	8000.530883	11.478119	-0.057022	4.816217
277.619834	8000.424363	11.483123	-0.057025	4.816186
277.457085	8000.574203	11.488128	-0.056995	4.816230
277.476654	8000.513668	11.493133	-0.056999	4.816212
277.520863	8000.456785	11.498138	-0.057007	4.816196
277.447381	8000.529182	11.503143	-0.056994	4.816217
277.404707	8000.542306	11.508147	-0.056986	4.816221
277.417667	8000.528662	11.513152	-0.056988	4.816217
277.468660	8000.494339	11.518157	-0.056998	4.816207
277.403311	8000.601073	11.523162	-0.056986	4.816238
277.610193	8000.601633	11.528167	-0.057025	4.816237
277.760532	8000.499665	11.533171	-0.057053	4.816207
277.513187	8000.575317	11.538176	-0.057007	4.816230
277.644945	8000.542460	11.543181	-0.057031	4.816220
277.745944	8000.644736	11.548186	-0.057050	4.816249
277.533500	8000.487035	11.553191	-0.057011	4.816204
277.694232	8000.514536	11.558195	-0.057041	4.816212
277.682907	8000.515409	11.563200	-0.057039	4.816212
277.454652	8000.563628	11.568205	-0.056996	4.816227
277.434514	8000.530151	11.573210	-0.056993	4.816217
277.397551	8000.618169	11.578215	-0.056986	4.816243
277.487322	8000.455270	11.583219	-0.057003	4.816195
277.458360	8000.592581	11.588224	-0.056997	4.816236
277.484628	8000.496909	11.593229	-0.057002	4.816207
277.514656	8000.434427	11.598234	-0.057008	4.816189
277.538690	8000.557741	11.603239	-0.057013	4.816225
277.727029	8000.444711	11.608243	-0.057048	4.816191
277.674363	8000.662793	11.613248	-0.057038	4.816255
277.596210	8000.393208	11.618253	-0.057024	4.816177
277.487476	8000.567534	11.623258	-0.057004	4.816228
277.469538	8000.623845	11.628263	-0.057000	4.816245
277.631849	8000.537053	11.633267	-0.057031	4.816218
277.604414	8000.597465	11.638272	-0.057026	4.816236
277.673303	8000.510045	11.643277	-0.057038	4.816210
277.775968	8000.570682	11.648282	-0.057058	4.816227
277.641639	8000.535132	11.653287	-0.057033	4.816218
277.614783	8000.377596	11.658291	-0.057028	4.816172
277.758547	8000.537273	11.663296	-0.057055	4.816218
277.700237	8000.541567	11.668301	-0.057044	4.816219
277.653536	8000.567439	11.673306	-0.057035	4.816227
277.524315	8000.531982	11.678311	-0.057011	4.816217
277.562274	8000.531612	11.683315	-0.057019	4.816217
277.747469	8000.530710	11.688320	-0.057053	4.816216
277.665410	8000.464056	11.693325	-0.057038	4.816197
277.716381	8000.630597	11.698330	-0.057048	4.816245
277.654066	8000.521564	11.703335	-0.057036	4.816214
277.678890	8000.531640	11.708339	-0.057041	4.816217
277.596774	8000.630592	11.713344	-0.057026	4.816246
277.539377	8000.516305	11.718349	-0.057015	4.816213
277.569455	8000.559598	11.723354	-0.057021	4.816225
277.574720	8000.566114	11.728359	-0.057022	4.816227
277.534856	8000.532279	11.733363	-0.057014	4.816217
277.511822	8000.645124	11.738368	-0.057010	4.816251
277.669664	8000.450339	11.743373	-0.057040	4.816193
277.629265	8000.554321	11.748378	-0.057032	4.816223
277.493637	8000.545458	11.753383	-0.057007	4.816222
277.535369	8000.515241	11.758387	-0.057015	4.816212
277.634759	8000.598255	11.763392	-0.057034	4.816236
277.740204	8000.508294	11.768397	-0.057053	4.816209
277.753901	8000.516031	11.773402	-0.057056	4.816212
277.608944	8000.620253	11.778407	-0.057029	4.816243
277.774851	8000.538868	11.783411	-0.057060	4.816218
277.775659	8000.471581	11.788416	-0.057060	4.816198
277.622375	8000.619457	11.793421	-0.057032	4.816242
277.780127	8000.555019	11.798426	-0.057061	4.816223
277.723681	8000.588194	11.803431	-0.057051	4.816233
277.884479	8000.439405	11.808435	-0.057081	4.816188
277.711848	8000.636078	11.813440	-0.057049	4.816247
277.828003	8000.599732	11.818445	-0.057071	4.816236
277.730226	8000.540271	11.823450	-0.057053	4.816219
277.656344	8000.592361	11.828455	-0.057039	4.816234
277.772582	8000.510075	11.833459	-0.057061	4.816210
277.678386	8000.587438	11.838464	-0.057043	4.816233
277.578405	8000.566401	11.843469	-0.057025	4.816227
277.622239	8000.534085	11.848474	-0.057033	4.816217
277.546284	8000.527374	11.853479	-0.057019	4.816216
277.651277	8000.663912	11.858483	-0.057039	4.816255
277.709777	8000.535703	11.863488	-0.057050	4.816217
277.909317	8000.560704	11.868493	-0.057087	4.816224
277.885470	8000.523953	11.873498	-0.057083	4.816213
277.701323	8000.597547	11.878503	-0.057048	4.816236
277.653525	8000.480230	11.883507	-0.057040	4.816202
277.638032	8000.616718	11.888512	-0.057037	4.816242
277.659767	8000.453652	11.893517	-0.057041	4.816194
277.549707	8000.520043	11.898522	-0.057020	4.816214
277.616423	8000.552248	11.903527	-0.057033	4.816223
277.746635	8000.467010	11.908531	-0.057057	4.816197
277.552376	8000.622690	11.913536	-0.057021	4.816244
277.799545	8000.580175	11.918541	-0.057067	4.816230
277.698441	8000.565528	11.923546	-0.057049	4.816226
277.683269	8000.512909	11.928551	-0.057046	4.816211
277.835644	8000.525301	11.933555	-0.057074	4.816214
277.896559	8000.605481	11.938560	-0.057086	4.816237
277.723829	8000.500853	11.943565	-0.057054	4.816207
277.720670	8000.646112	11.948570	-0.057053	4.816250
277.654838	8000.486799	11.953575	-0.057041	4.816203
277.602460	8000.615138	11.958579	-0.057032	4.816241
277.611392	8000.606762	11.963584	-0.057033	4.816239
277.588002	8000.477067	11.968589	-0.057029	4.816201
277.757147	8000.653233	11.973594	-0.057061	4.816251
277.559661	8000.510761	11.978599	-0.057024	4.816211
277.677786	8000.593048	11.983603	-0.057046	4.816234
277.741178	8000.534376	11.988608	-0.057058	4.816217
277.660118	8000.496587	11.993613	-0.057043	4.816206
277.705988	8000.548714	11.998618	-0.057052	4.816221
277.578878	8000.471626	12.003623	-0.057028	4.816199
277.711018	8000.501813	12.008627	-0.057053	4.816207
277.631836	8000.511070	12.013632	-0.057038	4.816211
277.635466	8000.498324	12.018637	-0.057039	4.816207
277.835770	8000.567145	12.023642	-0.057076	4.816226
277.720860	8000.582163	12.028647	-0.057055	4.816231
277.967340	8000.526815	12.033651	-0.057101	4.816213
277.944070	8000.572345	12.038656	-0.057097	4.816227
277.955672	8000.535170	12.043661	-0.057099	4.816216
277.859713	8000.502453	12.048666	-0.057081	4.816207
277.781123	8000.552320	12.053671	-0.057067	4.816222
277.664813	8000.533123	12.058675	-0.057045	4.816217
277.681714	8000.636010	12.063680	-0.057048	4.816247
277.769772	8000.461326	12.068685	-0.057065	4.816195
277.821424	8000.530653	12.073690	-0.057075	4.816215
277.812424	8000.578579	12.078695	-0.057073	4.816229
277.965072	8000.505501	12.083699	-0.057101	4.816207
278.016863	8000.625048	12.088704	-0.057111	4.816242
277.954298	8000.587594	12.093709	-0.057100	4.816231
277.905718	8000.558942	12.098714	-0.057091	4.816223
277.871752	8000.539103	12.103719	-0.057084	4.816217
277.872511	8000.418394	12.108723	-0.057085	4.816182
277.863444	8000.635131	12.113728	-0.057083	4.816246
277.906454	8000.463903	12.118733	-0.057091	4.816195
277.832973	8000.521343	12.123738	-0.057078	4.816212
277.893955	8000.582292	12.128743	-0.057089	4.816230
277.829503	8000.499930	12.133747	-0.057077	4.816206
277.837714	8000.585564	12.138752	-0.057079	4.816231
277.796099	8000.558107	12.143757	-0.057071	4.816223
277.680871	8000.529314	12.148762	-0.057050	4.816216
277.619616	8000.589112	12.153767	-0.057039	4.816233
277.855288	8000.627590	12.158771	-0.057083	4.816243
277.799527	8000.540044	12.163776	-0.057072	4.816218
277.734821	8000.582685	12.168781	-0.057060	4.816231
277.940588	8000.550103	12.173786	-0.057099	4.816220
277.845692	8000.430862	12.178791	-0.057081	4.816186
277.790661	8000.613643	12.183795	-0.057071	4.816240
277.799773	8000.509112	12.188800	-0.057073	4.816209
277.855434	8000.593470	12.193805	-0.057083	4.816233
277.797086	8000.533656	12.198810	-0.057072	4.816216
277.823275	8000.602521	12.203815	-0.057077	4.816236
277.773303	8000.492643	12.208819	-0.057068	4.816204
277.659314	8000.529047	12.213824	-0.057047	4.816216
277.797172	8000.602076	12.218829	-0.057073	4.816236
277.922605	8000.549872	12.223834	-0.057096	4.816220
277.870156	8000.504055	12.228839	-0.057087	4.816207
277.890866	8000.551452	12.233843	-0.057091	4.816221
277.942590	8000.645355	12.238848	-0.057100	4.816248
277.877595	8000.486056	12.243853	-0.057088	4.816202
277.862042	8000.534931	12.248858	-0.057086	4.816216
277.839243	8000.498200	12.253863	-0.057081	4.816206
278.007706	8000.524774	12.258867	-0.057113	4.816212
277.958535	8000.537780	12.263872	-0.057104	4.816217
277.937578	8000.536341	12.268877	-0.057100	4.816216
278.046286	8000.546872	12.273882	-0.057120	4.816219
277.845280	8000.594517	12.278887	-0.057083	4.816234
277.762318	8000.538530	12.283891	-0.057068	4.816218
277.786254	8000.532563	12.288896	-0.057072	4.816216
278.073153	8000.493976	12.293901	-0.057126	4.816203
278.105940	8000.519155	12.298906	-0.057132	4.816210
277.896625	8000.635029	12.303911	-0.057093	4.816245
278.017361	8000.412859	12.308915	-0.057116	4.816180
278.131919	8000.369005	12.313920	-0.057137	4.816166
277.911369	8000.558398	12.318925	-0.057096	4.816223
277.929957	8000.433738	12.323930	-0.057100	4.816186
277.826421	8000.597476	12.328935	-0.057081	4.816235
277.969215	8000.547724	12.333939	-0.057107	4.816219
277.699763	8000.472325	12.338944	-0.057057	4.816199
277.910460	8000.610783	12.343949	-0.057096	4.816238
278.066640	8000.531358	12.348954	-0.057126	4.816214
277.918685	8000.496628	12.353959	-0.057098	4.816205
278.192747	8000.353101	12.358963	-0.057149	4.816161
277.993948	8000.548231	12.363968	-0.057112	4.816219
277.980270	8000.607825	12.368973	-0.057110	4.816237
278.058245	8000.439368	12.373978	-0.057124	4.816187
277.984195	8000.614326	12.378983	-0.057111	4.816239
277.985239	8000.524605	12.383987	-0.057111	4.816212
278.036809	8000.565083	12.388992	-0.057121	4.816224
278.004834	8000.590155	12.393997	-0.057115	4.816232
277.994707	8000.510916	12.399002	-0.057113	4.816208
277.742063	8000.611046	12.404007	-0.057066	4.816239
277.787738	8000.494357	12.409011	-0.057075	4.816205
277.785310	8000.625740	12.414016	-0.057075	4.816243
277.959514	8000.486810	12.419021	-0.057107	4.816202
277.916282	8000.539456	12.424026	-0.057099	4.816217
277.800024	8000.467907	12.429031	-0.057077	4.816197
277.907737	8000.448503	12.434035	-0.057098	4.816191
277.773139	8000.512313	12.439040	-0.057073	4.816210
278.000223	8000.557045	12.444045	-0.057115	4.816222
277.983431	8000.525765	12.449050	-0.057112	4.816213
278.018265	8000.594788	12.454055	-0.057119	4.816233
278.175025	8000.417077	12.459059	-0.057148	4.816180
278.149794	8000.566210	12.464064	-0.057143	4.816224
277.823466	8000.483367	12.469069	-0.057083	4.816201
277.950554	8000.572228	12.474074	-0.057106	4.816227
277.885425	8000.548618	12.479079	-0.057094	4.816220
277.698104	8000.518516	12.484083	-0.057060	4.816212
277.647623	8000.613768	12.489088	-0.057050	4.816240
277.936718	8000.449144	12.494093	-0.057104	4.816191
277.987236	8000.505630	12.499098	-0.057114	4.816207
277.882977	8000.606317	12.504103	-0.057094	4.816237
277.902250	8000.510517	12.509107	-0.057098	4.816209
277.944008	8000.644840	12.514112	-0.057106	4.816248
278.005169	8000.527363	12.519117	-0.057117	4.816213
278.034633	8000.514017	12.524122	-0.057123	4.816209
278.145602	8000.627160	12.529127	-0.057144	4.816242
278.004469	8000.499599	12.534131	-0.057118	4.816205
278.036130	8000.607028	12.539136	-0.057124	4.816236
278.030340	8000.508636	12.544141	-0.057123	4.816207
278.184713	8000.376824	12.549146	-0.057151	4.816168
278.054090	8000.644778	12.554151	-0.057127	4.816247
278.005198	8000.420596	12.559155	-0.057118	4.816182
278.045276	8000.593352	12.564160	-0.057126	4.816232
278.058363	8000.461112	12.569165	-0.057128	4.816193
278.138270	8000.616429	12.574170	-0.057143	4.816238
277.982591	8000.595448	12.579175	-0.057115	4.816233
278.091565	8000.530124	12.584179	-0.057135	4.816213
277.853063	8000.534351	12.589184	-0.057091	4.816216
277.953647	8000.478491	12.594189	-0.057109	4.816199
278.190719	8000.483873	12.599194	-0.057154	4.816199
277.881149	8000.508179	12.604199	-0.057096	4.816208
278.088799	8000.461742	12.609203	-0.057135	4.816193
278.178298	8000.638601	12.614208	-0.057152	4.816245
278.016384	8000.535237	12.619213	-0.057122	4.816215
278.096602	8000.534566	12.624218	-0.057137	4.816215
277.916350	8000.580451	12.629223	-0.057103	4.816229
277.827798	8000.490173	12.634227	-0.057087	4.816203
277.911814	8000.541924	12.639232	-0.057102	4.816218
277.983567	8000.609480	12.644237	-0.057116	4.816237
278.030709	8000.537691	12.649242	-0.057125	4.816216
277.805871	8000.530414	12.654247	-0.057083	4.816215
277.963283	8000.525802	12.659251	-0.057112	4.816213
278.092032	8000.521738	12.664256	-0.057137	4.816211
278.065061	8000.614213	12.669261	-0.057132	4.816238
278.143201	8000.540850	12.674266	-0.057146	4.816216
278.072833	8000.494708	12.679271	-0.057133	4.816203
278.256618	8000.597420	12.684275	-0.057168	4.816232
278.009845	8000.502131	12.689280	-0.057122	4.816206
277.949750	8000.507460	12.694285	-0.057111	4.816207
278.065763	8000.511713	12.699290	-0.057132	4.816208
277.947501	8000.541628	12.704295	-0.057110	4.816217
277.971227	8000.565574	12.709299	-0.057115	4.816224
278.073076	8000.544996	12.714304	-0.057134	4.816218
278.060498	8000.604610	12.719309	-0.057132	4.816235
278.098321	8000.261270	12.724314	-0.057139	4.816135
277.999190	8000.603516	12.729319	-0.057121	4.816235
278.150606	8000.433187	12.734323	-0.057149	4.816185
278.069835	8000.522548	12.739328	-0.057134	4.816211
278.064502	8000.622894	12.744333	-0.057133	4.816241
278.203755	8000.379690	12.749338	-0.057159	4.816169
278.154083	8000.528380	12.754343	-0.057150	4.816212
278.092670	8000.535822	12.759347	-0.057139	4.816215
277.986967	8000.555281	12.764352	-0.057119	4.816221
277.914001	8000.495202	12.769357	-0.057105	4.816204
278.026464	8000.563496	12.774362	-0.057126	4.816223
278.035992	8000.519873	12.779367	-0.057128	4.816211
278.145763	8000.526149	12.784371	-0.057149	4.816212
277.946934	8000.535370	12.789376	-0.057112	4.816216
278.004331	8000.655019	12.794381	-0.057123	4.816250
278.062903	8000.551385	12.799386	-0.057134	4.816220
278.148993	8000.557231	12.804391	-0.057150	4.816221
278.079975	8000.476923	12.809395	-0.057137	4.816198
278.045126	8000.529722	12.814400	-0.057131	4.816213
278.205622	8000.497387	12.819405	-0.057161	4.816203
278.170320	8000.619627	12.824410	-0.057154	4.816239
277.932294	8000.622793	12.829415	-0.057110	4.816241
277.971562	8000.450429	12.834419	-0.057117	4.816191
278.006524	8000.602791	12.839424	-0.057124	4.816235
277.928483	8000.480650	12.844429	-0.057110	4.816200
278.135228	8000.595532	12.849434	-0.057148	4.816232
278.067869	8000.587907	12.854439	-0.057136	4.816230
278.156768	8000.389732	12.859443	-0.057152	4.816172
278.349531	8000.524660	12.864448	-0.057188	4.816210
278.385985	8000.497552	12.869453	-0.057195	4.816202
278.258520	8000.551875	12.874458	-0.057172	4.816219
278.014764	8000.635071	12.879463	-0.057126	4.816244
278.199023	8000.467475	12.884467	-0.057161	4.816194
278.319012	8000.533770	12.889472	-0.057183	4.816213
278.343880	8000.583380	12.894477	-0.057188	4.816227
278.362532	8000.537785	12.899482	-0.057192	4.816214
278.271588	8000.591702	12.904487	-0.057175	4.816230
278.055712	8000.404020	12.909491	-0.057134	4.816177
278.146465	8000.634324	12.914496	-0.057152	4.816243
278.210190	8000.503004	12.919501	-0.057164	4.816205
278.103551	8000.639975	12.924506	-0.057144	4.816245
277.971883	8000.532886	12.929511	-0.057119	4.816215
278.054301	8000.509818	12.934515	-0.057135	4.816207
278.101717	8000.614328	12.939520	-0.057144	4.816238
278.152561	8000.555427	12.944525	-0.057153	4.816220
278.338202	8000.479743	12.949530	-0.057188	4.816197
278.406313	8000.614546	12.954535	-0.057201	4.816236
278.107907	8000.540756	12.959539	-0.057145	4.816216
278.154013	8000.510617	12.964544	-0.057154	4.816207
278.311690	8000.534859	12.969549	-0.057183	4.816213
278.240484	8000.563492	12.974554	-0.057170	4.816222
277.989509	8000.568561	12.979559	-0.057124	4.816225
278.049559	8000.469227	12.984563	-0.057135	4.816196
277.974045	8000.515945	12.989568	-0.057121	4.816210
277.998157	8000.571952	12.994573	-0.057126	4.816226
278.141438	8000.532893	12.999578	-0.057152	4.816214
278.130784	8000.611775	13.004583	-0.057150	4.816237
278.073274	8000.529538	13.009587	-0.057140	4.816213
277.988109	8000.646599	13.014592	-0.057124	4.816248
278.161744	8000.438209	13.019597	-0.057156	4.816186
278.046467	8000.528012	13.024602	-0.057135	4.816213
277.975055	8000.578010	13.029607	-0.057122	4.816228
278.147332	8000.577942	13.034611	-0.057154	4.816227
278.222299	8000.505590	13.039616	-0.057168	4.816205
278.009627	8000.540202	13.044621	-0.057129	4.816217
278.102550	8000.427576	13.049626	-0.057146	4.816183
278.072566	8000.579828	13.054631	-0.057141	4.816228
277.973846	8000.572703	13.059635	-0.057122	4.816226
278.187667	8000.514625	13.064640	-0.057162	4.816208
278.185021	8000.603268	13.069645	-0.057162	4.816234
278.057630	8000.546474	13.074650	-0.057138	4.816218
277.974508	8000.521468	13.079655	-0.057123	4.816211
278.202449	8000.530959	13.084659	-0.057165	4.816213
278.235891	8000.541192	13.089664	-0.057172	4.816216
278.242069	8000.563751	13.094669	-0.057173	4.816222
278.400746	8000.519630	13.099674	-0.057203	4.816208
278.537624	8000.573411	13.104679	-0.057228	4.816223
278.527265	8000.500577	13.109683	-0.057226	4.816202
278.368910	8000.615241	13.114688	-0.057197	4.816237
278.538166	8000.587340	13.119693	-0.057229	4.816227
278.507871	8000.461790	13.124698	-0.057223	4.816191
278.339610	8000.592301	13.129703	-0.057192	4.816230
278.631059	8000.518537	13.134707	-0.057246	4.816207
278.486716	8000.642003	13.139712	-0.057219	4.816244
278.301060	8000.555302	13.144717	-0.057185	4.816219
278.346372	8000.542244	13.149722	-0.057193	4.816215
278.394877	8000.590147	13.154727	-0.057203	4.816229
278.513844	8000.514320	13.159731	-0.057225	4.816206
278.336324	8000.505763	13.164736	-0.057192	4.816205
278.264751	8000.519432	13.169741	-0.057179	4.816209
278.403320	8000.531573	13.174746	-0.057204	4.816212
278.111354	8000.623510	13.179751	-0.057150	4.816240
278.370712	8000.489331	13.184755	-0.057199	4.816200
278.525553	8000.523137	13.189760	-0.057228	4.816209
278.529932	8000.588402	13.194765	-0.057229	4.816228
278.335975	8000.358379	13.199770	-0.057192	4.816162
278.431597	8000.417820	13.204775	-0.057210	4.816178
278.426818	8000.449796	13.209779	-0.057210	4.816188
278.468407	8000.617240	13.214784	-0.057217	4.816237
278.508405	8000.528226	13.219789	-0.057225	4.816210
278.433191	8000.549307	13.224794	-0.057211	4.816217
278.314756	8000.523660	13.229799	-0.057189	4.816210
278.241798	8000.483881	13.234803	-0.057176	4.816199
278.451906	8000.573182	13.239808	-0.057215	4.816224
278.367261	8000.571654	13.244813	-0.057199	4.816224
278.315717	8000.536537	13.249818	-0.057190	4.816214
278.283499	8000.533825	13.254823	-0.057184	4.816213
278.524333	8000.587357	13.259827	-0.057229	4.816227
278.336506	8000.521985	13.264832	-0.057194	4.816209
278.278765	8000.543384	13.269837	-0.057183	4.816216
278.291650	8000.610940	13.274842	-0.057186	4.816236
278.299097	8000.533087	13.279847	-0.057187	4.816213
278.210114	8000.498359	13.284851	-0.057171	4.816203
278.323426	8000.623299	13.289856	-0.057192	4.816239
278.408400	8000.461378	13.294861	-0.057208	4.816191
278.363002	8000.526807	13.299866	-0.057199	4.816211
278.177230	8000.645247	13.304871	-0.057165	4.816246
278.483816	8000.333494	13.309875	-0.057222	4.816153
278.214316	8000.406607	13.314880	-0.057172	4.816176
278.254184	8000.512048	13.319885	-0.057180	4.816207
278.591548	8000.478651	13.324890	-0.057242	4.816195
278.428182	8000.513090	13.329895	-0.057212	4.816206
278.211217	8000.509160	13.334899	-0.057172	4.816206
278.187064	8000.552537	13.339904	-0.057167	4.816219
278.235876	8000.587624	13.344909	-0.057177	4.816229
278.437399	8000.525048	13.349914	-0.057214	4.816210
278.309548	8000.539832	13.354919	-0.057191	4.816215
278.324937	8000.543326	13.359923	-0.057194	4.816216
278.345135	8000.550113	13.364928	-0.057197	4.816217
278.333009	8000.465495	13.369933	-0.057195	4.816193
278.590668	8000.517195	13.374938	-0.057243	4.816207
278.549981	8000.613696	13.379943	-0.057236	4.816235
278.403399	8000.515951	13.384947	-0.057209	4.816207
278.244168	8000.536575	13.389952	-0.057179	4.816214
278.126931	8000.498128	13.394957	-0.057157	4.816203
278.249659	8000.612554	13.399962	-0.057180	4.816236
278.221415	8000.544738	13.404967	-0.057175	4.816217
278.500181	8000.479292	13.409971	-0.057227	4.816196
278.468120	8000.573811	13.414976	-0.057221	4.816224
278.352723	8000.495865	13.419981	-0.057200	4.816202
278.369568	8000.532508	13.424986	-0.057203	4.816212
278.371356	8000.521866	13.429991	-0.057204	4.816209
278.358026	8000.519496	13.434995	-0.057201	4.816208
278.422136	8000.382840	13.440000	-0.057213	4.816168
278.584418	8000.558886	13.445005	-0.057244	4.816219
278.576498	8000.425195	13.450010	-0.057242	4.816180
278.622657	8000.537162	13.455015	-0.057251	4.816212
278.545279	8000.472727	13.460019	-0.057236	4.816194
278.480648	8000.449126	13.465024	-0.057225	4.816187
278.360496	8000.599742	13.470029	-0.057202	4.816232
278.449433	8000.525507	13.475034	-0.057219	4.816210
278.383388	8000.591630	13.480039	-0.057207	4.816229
278.397148	8000.536329	13.485043	-0.057209	4.816213
278.576756	8000.522505	13.490048	-0.057243	4.816208
278.547570	8000.581818	13.495053	-0.057238	4.816226
278.432031	8000.551950	13.500058	-0.057216	4.816217
278.179315	8000.545234	13.505063	-0.057169	4.816217
278.412922	8000.507815	13.510067	-0.057213	4.816205
278.417918	8000.389318	13.515072	-0.057214	4.816170
278.162792	8000.517183	13.520077	-0.057166	4.816209
278.290329	8000.604984	13.525082	-0.057190	4.816234
278.612503	8000.562764	13.530087	-0.057250	4.816220
278.572474	8000.493665	13.535091	-0.057243	4.816200
278.452726	8000.513938	13.540096	-0.057221	4.816206
278.520407	8000.629502	13.545101	-0.057234	4.816240
278.580580	8000.427597	13.550106	-0.057245	4.816180
278.498341	8000.546849	13.555111	-0.057230	4.816216
278.411563	8000.443780	13.560115	-0.057214	4.816186
278.278458	8000.537533	13.565120	-0.057189	4.816214
278.307124	8000.549816	13.570125	-0.057194	4.816217
278.334544	8000.513996	13.575130	-0.057200	4.816207
278.360273	8000.542252	13.580135	-0.057204	4.816215
278.343361	8000.432973	13.585139	-0.057201	4.816183
278.429215	8000.498649	13.590144	-0.057217	4.816202
278.671198	8000.523353	13.595149	-0.057263	4.816208
278.644282	8000.450219	13.600154	-0.057258	4.816187
278.226790	8000.627490	13.605159	-0.057180	4.816241
278.570123	8000.512999	13.610163	-0.057244	4.816205
278.515058	8000.525898	13.615168	-0.057234	4.816209
278.276402	8000.536532	13.620173	-0.057190	4.816214
278.427748	8000.461293	13.625178	-0.057218	4.816191
278.444473	8000.629354	13.630183	-0.057221	4.816240
278.518605	8000.488605	13.635187	-0.057235	4.816198
278.283352	8000.560203	13.640192	-0.057191	4.816221
278.229951	8000.538942	13.645197	-0.057181	4.816215
278.334794	8000.598552	13.650202	-0.057201	4.816232
278.243772	8000.555239	13.655207	-0.057184	4.816219
278.342747	8000.502555	13.660211	-0.057203	4.816203
278.358457	8000.511397	13.665216	-0.057206	4.816206
278.386323	8000.632648	13.670221	-0.057211	4.816241
278.395495	8000.540937	13.675226	-0.057213	4.816214
278.415191	8000.556263	13.680231	-0.057217	4.816219
278.576020	8000.496154	13.685235	-0.057247	4.816200
278.558161	8000.522551	13.690240	-0.057243	4.816208
278.549086	8000.561929	13.695245	-0.057242	4.816220
278.565414	8000.529113	13.700250	-0.057245	4.816210
278.409611	8000.633138	13.705255	-0.057216	4.816241
278.415161	8000.491144	13.710259	-0.057217	4.816200
278.610116	8000.426313	13.715264	-0.057254	4.816180
278.285776	8000.553989	13.720269	-0.057193	4.816219
278.326889	8000.356014	13.725274	-0.057201	4.816161
278.519240	8000.563591	13.730279	-0.057237	4.816220
278.490199	8000.551320	13.735283	-0.057232	4.816217
278.301778	8000.476321	13.740288	-0.057197	4.816196
278.306089	8000.553338	13.745293	-0.057198	4.816218
278.662337	8000.528832	13.750298	-0.057264	4.816209
278.537087	8000.571442	13.755303	-0.057241	4.816222
278.423087	8000.476426	13.760307	-0.057220	4.816195
278.608091	8000.530012	13.765312	-0.057254	4.816210
278.449920	8000.569888	13.770317	-0.057225	4.816222
278.524011	8000.508204	13.775322	-0.057239	4.816204
278.462861	8000.620359	13.780327	-0.057228	4.816237
278.510808	8000.498367	13.785331	-0.057236	4.816201
278.537772	8000.555494	13.790336	-0.057242	4.816218
278.451562	8000.559281	13.795341	-0.057226	4.816219
278.641117	8000.435586	13.800346	-0.057261	4.816182
278.484300	8000.604770	13.805351	-0.057232	4.816232
278.363369	8000.476506	13.810355	-0.057210	4.816196
278.391459	8000.615924	13.815360	-0.057215	4.816236
278.284939	8000.456937	13.820365	-0.057195	4.816190
278.132598	8000.522561	13.825370	-0.057167	4.816210
278.420926	8000.524601	13.830375	-0.057221	4.816209
278.416926	8000.513853	13.835379	-0.057220	4.816206
278.307454	8000.614447	13.840384	-0.057200	4.816236
278.332685	8000.515548	13.845389	-0.057205	4.816207
278.542685	8000.546083	13.850394	-0.057244	4.816215
278.430488	8000.489563	13.855399	-0.057223	4.816199
278.180238	8000.504261	13.860403	-0.057176	4.816205
278.360708	8000.626146	13.865408	-0.057210	4.816239
278.448627	8000.513428	13.870413	-0.057227	4.816206
278.352208	8000.589684	13.875418	-0.057209	4.816229
278.429249	8000.568655	13.880423	-0.057223	4.816222
278.419350	8000.506514	13.885427	-0.057221	4.816204
278.341879	8000.536102	13.890432	-0.057207	4.816213
278.221909	8000.529659	13.895437	-0.057185	4.816212
278.386971	8000.495270	13.900442	-0.057216	4.816201
278.333182	8000.592601	13.905447	-0.057206	4.816230
278.307995	8000.579332	13.910451	-0.057201	4.816226
278.438238	8000.537900	13.915456	-0.057226	4.816213
278.566560	8000.521007	13.920461	-0.057250	4.816207
278.630076	8000.516828	13.925466	-0.057261	4.816206
278.459124	8000.525486	13.930471	-0.057230	4.816209
278.681814	8000.553046	13.935475	-0.057271	4.816216
278.653143	8000.554672	13.940480	-0.057266	4.816217
278.441680	8000.505966	13.945485	-0.057227	4.816204
278.416797	8000.518345	13.950490	-0.057222	4.816207
278.297280	8000.539690	13.955495	-0.057200	4.816214
278.384553	8000.559449	13.960499	-0.057216	4.816220
278.324929	8000.579745	13.965504	-0.057205	4.816226
278.407018	8000.523548	13.970509	-0.057221	4.816209
278.488946	8000.498334	13.975514	-0.057236	4.816201
278.341152	8000.574726	13.980519	-0.057209	4.816224
278.391292	8000.574577	13.985523	-0.057218	4.816224
278.428454	8000.517565	13.990528	-0.057225	4.816207
278.409132	8000.557825	13.995533	-0.057222	4.816219
278.431594	8000.561448	14.000538	-0.057226	4.816220
278.488541	8000.510137	14.005543	-0.057237	4.816205
278.317863	8000.612825	14.010547	-0.057205	4.816236
278.549995	8000.450371	14.015552	-0.057248	4.816187
278.537675	8000.578371	14.020557	-0.057246	4.816224
278.572090	8000.535199	14.025562	-0.057253	4.816212
278.528450	8000.517321	14.030567	-0.057245	4.816207
278.596299	8000.472619	14.035571	-0.057257	4.816193
278.758778	8000.547166	14.040576	-0.057288	4.816214
278.398151	8000.525668	14.045581	-0.057221	4.816210
278.420526	8000.411760	14.050586	-0.057225	4.816176
278.421152	8000.643635	14.055591	-0.057225	4.816244
278.322667	8000.427097	14.060595	-0.057207	4.816181
278.272411	8000.547997	14.065600	-0.057198	4.816217
278.422379	8000.484486	14.070605	-0.057226	4.816197
278.498061	8000.596990	14.075610	-0.057240	4.816230
278.486969	8000.509184	14.080615	-0.057238	4.816204
278.626713	8000.544854	14.085619	-0.057264	4.816214
278.589001	8000.629655	14.090624	-0.057257	4.816239
278.535275	8000.462010	14.095629	-0.057247	4.816190
278.591310	8000.611553	14.100634	-0.057258	4.816234
278.572680	8000.513994	14.105639	-0.057254	4.816205
278.532539	8000.506864	14.110643	-0.057247	4.816203
278.465928	8000.524896	14.115648	-0.057235	4.816209
278.595321	8000.479175	14.120653	-0.057259	4.816195
278.617113	8000.524455	14.125658	-0.057263	4.816208
278.449099	8000.599411	14.130663	-0.057232	4.816231
278.427969	8000.519971	14.135667	-0.057228	4.816208
278.596246	8000.629883	14.140672	-0.057259	4.816239
278.596485	8000.552967	14.145677	-0.057260	4.816217
278.685321	8000.515057	14.150682	-0.057276	4.816205
278.576676	8000.499204	14.155687	-0.057256	4.816201
278.482626	8000.587256	14.160691	-0.057239	4.816227
278.329372	8000.539607	14.165696	-0.057210	4.816214
278.431011	8000.586338	14.170701	-0.057229	4.816227
278.623115	8000.572741	14.175706	-0.057265	4.816222
278.607057	8000.556432	14.180711	-0.057262	4.816217
278.516184	8000.522737	14.185715	-0.057245	4.816208
278.716461	8000.613998	14.190720	-0.057283	4.816234
278.436767	8000.583285	14.195725	-0.057231	4.816226
278.451350	8000.435044	14.200730	-0.057234	4.816183
278.392262	8000.624166	14.205735	-0.057223	4.816238
278.358412	8000.488935	14.210739	-0.057216	4.816199
278.481050	8000.501856	14.215744	-0.057239	4.816202
278.498138	8000.491492	14.220749	-0.057243	4.816199
278.603295	8000.633379	14.225754	-0.057262	4.816240
278.442855	8000.542861	14.230759	-0.057233	4.816214
278.611532	8000.553413	14.235763	-0.057264	4.816217
278.792969	8000.450940	14.240768	-0.057298	4.816186
278.646886	8000.577581	14.245773	-0.057271	4.816223
278.554726	8000.552410	14.250778	-0.057254	4.816217
278.474167	8000.535998	14.255783	-0.057239	4.816212
278.661215	8000.469955	14.260787	-0.057274	4.816192
278.713787	8000.328815	14.265792	-0.057284	4.816150
278.582955	7999.511245	14.270797	-0.057259	4.815912

278.608168	7996.251296	14.275802	-0.057261	4.814959
278.506729	7990.718303	14.280807	-0.057239	4.813342
278.461150	7983.993750	14.285811	-0.057226	4.811376
278.482871	7976.686343	14.290816	-0.057226	4.809238
278.172125	7968.977562	14.295821	-0.057163	4.806984
278.217499	7961.244538	14.300826	-0.057166	4.804719
278.471813	7953.397251	14.305831	-0.057209	4.802419
278.425113	7945.413335	14.310835	-0.057195	4.800079
278.012455	7937.480475	14.315840	-0.057113	4.797754
277.952369	7929.384013	14.320845	-0.057097	4.795379
278.083265	7921.408465	14.325850	-0.057116	4.793037
277.977077	7913.414905	14.330855	-0.057091	4.790690
277.909975	7905.391939	14.335859	-0.057073	4.788333
278.034439	7897.427979	14.340864	-0.057092	4.785991
277.895316	7889.405440	14.345869	-0.057060	4.783632
277.840804	7881.430638	14.350874	-0.057045	4.781286
277.788390	7873.372880	14.355879	-0.057030	4.778914
277.770516	7865.431984	14.360883	-0.057022	4.776575
277.897084	7857.450511	14.365888	-0.057040	4.774222
277.947350	7849.390318	14.370893	-0.057045	4.771845
277.834621	7841.379416	14.375898	-0.057018	4.769482
277.671876	7833.399326	14.380903	-0.056983	4.767128
277.510760	7825.335543	14.385907	-0.056948	4.764747
277.499817	7817.450119	14.390912	-0.056941	4.762418
277.365472	7809.372608	14.395917	-0.056911	4.760030
277.429785	7801.430610	14.400922	-0.056918	4.757681
277.387722	7793.357154	14.405927	-0.056905	4.755293
277.302672	7785.312529	14.410931	-0.056884	4.752912
277.305916	7777.318414	14.415936	-0.056879	4.750544
277.334863	7769.361265	14.420941	-0.056879	4.748186
277.513337	7761.347795	14.425946	-0.056907	4.745809
277.286005	7753.384918	14.430951	-0.056860	4.743448
277.223356	7745.339723	14.435955	-0.056843	4.741061
277.234323	7737.369906	14.440960	-0.056840	4.738694
277.165692	7729.342218	14.445965	-0.056822	4.736310
277.054593	7721.337029	14.450970	-0.056796	4.733931
276.871536	7713.299427	14.455975	-0.056757	4.731541
276.896947	7705.274542	14.460979	-0.056757	4.729154
276.829775	7697.324012	14.465984	-0.056739	4.726787
276.708184	7689.322427	14.470989	-0.056712	4.724404
276.668240	7681.377107	14.475994	-0.056699	4.722037
276.842736	7673.317578	14.480999	-0.056726	4.719634
276.692827	7665.353036	14.486003	-0.056693	4.717258
276.687251	7657.356332	14.491008	-0.056687	4.714872
276.507301	7649.291979	14.496013	-0.056648	4.712465
276.546818	7641.278811	14.501018	-0.056651	4.710071
276.577874	7633.272765	14.506023	-0.056651	4.707678
276.578558	7625.284082	14.511027	-0.056646	4.705289
276.310746	7617.352391	14.516032	-0.056591	4.702916
276.319641	7609.308331	14.521037	-0.056588	4.700508
276.394082	7601.347110	14.526042	-0.056597	4.698124
276.300979	7593.305205	14.531047	-0.056574	4.695714
276.394271	7585.302282	14.536051	-0.056587	4.693315
276.457171	7577.292780	14.541056	-0.056593	4.690912
276.170048	7569.324217	14.546061	-0.056535	4.688521
275.917939	7561.262388	14.551066	-0.056482	4.686101
275.906137	7553.285528	14.556071	-0.056475	4.683704
276.105581	7545.291406	14.561075	-0.056507	4.681301
276.147005	7537.339677	14.566080	-0.056510	4.678910
275.762091	7529.271953	14.571085	-0.056433	4.676483
275.982654	7521.276763	14.576090	-0.056469	4.674075
275.888784	7513.169662	14.581095	-0.056446	4.671634
275.822824	7505.187153	14.586099	-0.056429	4.669228
275.624805	7497.232861	14.591104	-0.056387	4.666830
275.932379	7489.243191	14.596109	-0.056439	4.664419
275.864925	7481.283407	14.601114	-0.056421	4.662017
275.710361	7473.241516	14.606119	-0.056388	4.659589
275.706973	7465.263535	14.611123	-0.056382	4.657178
275.682212	7457.261714	14.616128	-0.056372	4.654759
275.459602	7449.237342	14.621133	-0.056325	4.652333
275.617937	7441.199370	14.626138	-0.056350	4.649900
275.546819	7433.216107	14.631143	-0.056331	4.647483
275.223672	7425.203027	14.636147	-0.056266	4.645056
275.355019	7417.278429	14.641152	-0.056286	4.642654
275.314213	7409.227566	14.646157	-0.056273	4.640212
275.147890	7401.303965	14.651162	-0.056237	4.637808
274.994798	7393.223170	14.656167	-0.056203	4.635355
274.964935	7385.204652	14.661171	-0.056192	4.632920
275.143323	7377.185847	14.666176	-0.056221	4.630483
275.043065	7369.197127	14.671181	-0.056197	4.628054
274.829672	7361.181582	14.676186	-0.056152	4.625616
274.960690	7353.246021	14.681191	-0.056171	4.623200
275.002106	7345.177035	14.686195	-0.056174	4.620743
274.975179	7337.217709	14.691200	-0.056164	4.618318
274.668051	7329.186325	14.696205	-0.056101	4.615869
274.793392	7321.188660	14.701210	-0.056120	4.613430
274.636429	7313.173321	14.706215	-0.056085	4.610984
274.683590	7305.176855	14.711219	-0.056089	4.608542
274.662575	7297.175355	14.716224	-0.056080	4.606098
274.427169	7289.161614	14.721229	-0.056031	4.603648
274.460369	7281.216691	14.726234	-0.056032	4.601218
274.622067	7273.220931	14.731239	-0.056057	4.598772
274.436698	7265.192601	14.736243	-0.056017	4.596314
274.306208	7257.151326	14.741248	-0.055988	4.593850
274.271093	7249.083855	14.746253	-0.055976	4.591378
274.353270	7241.142843	14.751258	-0.055986	4.588943
274.198869	7233.121727	14.756263	-0.055953	4.586481
274.151004	7225.119136	14.761267	-0.055939	4.584025
274.346616	7217.186677	14.766272	-0.055970	4.581588
274.119934	7209.143080	14.771277	-0.055923	4.579116
274.164512	7201.173595	14.776282	-0.055926	4.576666
274.210261	7193.131263	14.781287	-0.055929	4.574192
274.106988	7185.120911	14.786291	-0.055905	4.571726
273.935516	7177.156613	14.791296	-0.055868	4.569273
273.957663	7169.106106	14.796301	-0.055867	4.566792
274.121098	7161.130505	14.801306	-0.055892	4.564333
273.886762	7153.170272	14.806311	-0.055843	4.561878
273.906745	7145.146991	14.811315	-0.055842	4.559401
273.771925	7137.175012	14.816320	-0.055812	4.556939
273.597751	7129.114595	14.821325	-0.055774	4.554448
273.567134	7121.116742	14.826330	-0.055763	4.551976
273.650062	7113.110749	14.831335	-0.055774	4.549499
273.611153	7105.094415	14.836339	-0.055761	4.547018
273.430446	7097.126373	14.841344	-0.055723	4.544551
273.508464	7089.153619	14.846349	-0.055732	4.542081
273.697095	7081.157522	14.851354	-0.055762	4.539602
273.508427	7073.151318	14.856359	-0.055722	4.537119
273.309704	7065.113422	14.861363	-0.055680	4.534624
273.385135	7057.123930	14.866368	-0.055689	4.532143
273.082496	7049.082443	14.871373	-0.055627	4.529644
273.236024	7041.130469	14.876378	-0.055651	4.527172
273.114863	7033.095979	14.881383	-0.055623	4.524673
272.997934	7025.147198	14.886387	-0.055596	4.522199
273.020916	7017.127825	14.891392	-0.055595	4.519702
272.924035	7009.154683	14.896397	-0.055572	4.517218
272.975405	7001.115959	14.901402	-0.055576	4.514713
272.957100	6993.021093	14.906407	-0.055568	4.512188
273.027438	6985.012196	14.911411	-0.055576	4.509689
273.042270	6977.068074	14.916416	-0.055573	4.507208
272.648366	6969.031297	14.921421	-0.055495	4.504697
272.756846	6961.105369	14.926426	-0.055510	4.502219
272.777218	6953.075648	14.931431	-0.055509	4.499708
272.668441	6945.088296	14.936435	-0.055483	4.497208
272.749820	6937.061088	14.941440	-0.055493	4.494695
272.572724	6929.034438	14.946445	-0.055455	4.492180
272.682313	6921.053820	14.951450	-0.055471	4.489678
272.574675	6913.100337	14.956455	-0.055446	4.487184
272.301684	6905.046328	14.961459	-0.055390	4.484655
272.391711	6897.123009	14.966464	-0.055401	4.482168
272.250177	6889.003476	14.971469	-0.055370	4.479617
272.146970	6881.078916	14.976474	-0.055345	4.477125
272.085271	6873.039347	14.981479	-0.055329	4.474596
272.069677	6865.015815	14.986483	-0.055321	4.472071
272.078894	6857.029297	14.991488	-0.055317	4.469557
272.151651	6849.017916	14.996493	-0.055326	4.467033
271.967706	6841.039391	15.001498	-0.055286	4.464517
271.775884	6833.073443	15.006503	-0.055246	4.462004
271.820101	6825.004747	15.011507	-0.055249	4.459457
271.868221	6817.056250	15.016512	-0.055253	4.456948
271.869045	6808.990245	15.021517	-0.055248	4.454399
271.669463	6801.040683	15.026522	-0.055205	4.451885
271.768985	6793.009425	15.031527	-0.055219	4.449345
271.646013	6785.020788	15.036531	-0.055191	4.446816
271.704452	6777.035611	15.041536	-0.055196	4.444288
271.606535	6769.029246	15.046541	-0.055173	4.441751
271.539913	6761.086191	15.051546	-0.055156	4.439232
271.527071	6753.025014	15.056551	-0.055148	4.436675
271.387321	6745.032033	15.061555	-0.055117	4.434137
271.379309	6736.997795	15.066560	-0.055110	4.431586
271.335274	6728.986340	15.071565	-0.055097	4.429040
271.249400	6720.989880	15.076570	-0.055076	4.426497
271.154851	6712.994249	15.081575	-0.055053	4.423953
271.156686	6704.991178	15.086579	-0.055048	4.421405
271.209130	6697.027312	15.091584	-0.055053	4.418869
271.023293	6688.960644	15.096589	-0.055013	4.416297
271.038489	6680.980104	15.101594	-0.055011	4.413753
270.874316	6672.936296	15.106599	-0.054975	4.411185
270.801163	6664.928190	15.111603	-0.054957	4.408628
271.049452	6656.953277	15.116608	-0.054998	4.406082
270.877164	6648.990105	15.121613	-0.054961	4.403536
270.659934	6641.007891	15.126618	-0.054915	4.400982
270.601814	6633.030908	15.131623	-0.054899	4.398429
270.627196	6625.014407	15.136627	-0.054899	4.395863
270.740797	6616.987569	15.141632	-0.054915	4.393292
270.651945	6608.958858	15.146637	-0.054893	4.390718
270.451490	6600.989233	15.151642	-0.054851	4.388161
270.523411	6592.977136	15.156647	-0.054859	4.385590
270.335165	6585.014806	15.161651	-0.054819	4.383032
270.437051	6577.019364	15.166656	-0.054833	4.380463
270.288177	6569.013375	15.171661	-0.054800	4.377889
270.190661	6560.982184	15.176666	-0.054776	4.375304
270.245016	6553.011353	15.181671	-0.054781	4.372739
270.324660	6544.963344	15.186675	-0.054791	4.370148
270.413885	6536.984806	15.191680	-0.054803	4.367577
270.287600	6528.954756	15.196685	-0.054774	4.364987
270.136357	6521.056703	15.201690	-0.054741	4.362438
270.202240	6513.010506	15.206695	-0.054748	4.359841
270.080072	6505.009253	15.211699	-0.054720	4.357255
269.807762	6497.000142	15.216704	-0.054664	4.354665
269.732602	6488.861938	15.221709	-0.054645	4.352032
269.859037	6480.940914	15.226714	-0.054664	4.349470
269.852002	6472.934536	15.231719	-0.054657	4.346877
269.740945	6464.947481	15.236723	-0.054631	4.344289
269.810851	6457.024281	15.241728	-0.054639	4.341721
269.746947	6448.940972	15.246733	-0.054622	4.339098
269.629682	6440.968460	15.251738	-0.054595	4.336510
269.717375	6432.956276	15.256743	-0.054606	4.333908
269.442149	6424.912070	15.261747	-0.054550	4.331292
269.522534	6416.944255	15.266752	-0.054560	4.328702
269.582334	6408.922137	15.271757	-0.054566	4.326092
269.421289	6400.972732	15.276762	-0.054531	4.323503
269.427716	6392.982472	15.281767	-0.054527	4.320900
269.298801	6385.007573	15.286771	-0.054498	4.318300
269.270759	6376.970299	15.291776	-0.054488	4.315679
268.956465	6368.927876	15.296781	-0.054424	4.313052
269.106768	6360.916642	15.301786	-0.054447	4.310437
269.280814	6352.925931	15.306791	-0.054474	4.307827
269.166908	6344.884362	15.311795	-0.054448	4.305197
269.061225	6336.993543	15.316800	-0.054423	4.302615
269.090724	6328.886108	15.321805	-0.054423	4.299961
269.146675	6320.983170	15.326810	-0.054429	4.297373
268.900243	6312.923393	15.331815	-0.054378	4.294730
268.960279	6304.931035	15.336819	-0.054384	4.292109
268.929605	6296.904771	15.341824	-0.054373	4.289475
268.759910	6288.926665	15.346829	-0.054336	4.286854
268.759449	6280.920984	15.351834	-0.054331	4.284224
268.951230	6272.908013	15.356839	-0.054361	4.281591
268.650872	6264.926053	15.361843	-0.054300	4.278963
268.700079	6256.958606	15.366848	-0.054305	4.276341
268.641550	6248.911507	15.371853	-0.054288	4.273690
268.472662	6240.905315	15.376858	-0.054252	4.271050
268.346777	6232.887932	15.381863	-0.054223	4.268405
268.235898	6224.887495	15.386867	-0.054198	4.265764
268.263686	6216.916901	15.391872	-0.054198	4.263132
268.091208	6208.895891	15.396877	-0.054160	4.260481
268.250493	6200.908217	15.401882	-0.054185	4.257842
268.399068	6192.926661	15.406887	-0.054208	4.255203
268.335952	6184.865026	15.411891	-0.054191	4.252534
268.323109	6176.901391	15.416896	-0.054183	4.249896
268.261260	6168.911996	15.421901	-0.054167	4.247247
268.182331	6160.937485	15.426906	-0.054147	4.244602
268.032504	6152.949204	15.431911	-0.054114	4.241950
268.008516	6144.928734	15.436915	-0.054104	4.239287
268.085690	6136.957523	15.441920	-0.054113	4.236639
267.792034	6128.924506	15.446925	-0.054054	4.233965
267.881145	6120.888888	15.451930	-0.054065	4.231293
267.802113	6112.913644	15.456935	-0.054045	4.228637
267.836749	6104.887781	15.461939	-0.054047	4.225964
267.755874	6096.960154	15.466944	-0.054026	4.223321
267.675976	6088.917721	15.471949	-0.054006	4.220638
267.799548	6080.961573	15.476954	-0.054024	4.217984
267.671497	6072.912054	15.481959	-0.053995	4.215295
267.501421	6064.900711	15.486963	-0.053959	4.212616
267.479504	6056.917269	15.491968	-0.053949	4.209947
267.434286	6048.929333	15.496973	-0.053936	4.207274
267.333288	6040.942563	15.501978	-0.053912	4.204599
267.350655	6033.015148	15.506983	-0.053910	4.201943
267.312689	6024.938927	15.511987	-0.053898	4.199235
267.350028	6016.986614	15.516992	-0.053900	4.196568
267.341045	6008.863163	15.521997	-0.053893	4.193842
267.221679	6000.794853	15.527002	-0.053865	4.191130
267.089695	5992.858501	15.532007	-0.053836	4.188462
266.971477	5984.873945	15.537011	-0.053809	4.185775
267.084821	5976.928140	15.542016	-0.053825	4.183102
266.947854	5968.903490	15.547021	-0.053794	4.180399
266.851475	5960.921712	15.552026	-0.053771	4.177708
266.954734	5952.893412	15.557031	-0.053785	4.175002
266.801293	5944.889604	15.562035	-0.053751	4.172300
266.752512	5936.886755	15.567040	-0.053737	4.169598
266.647868	5928.886314	15.572045	-0.053713	4.166894
266.686816	5920.908590	15.577050	-0.053715	4.164197
266.564234	5912.943170	15.582055	-0.053687	4.161502
266.336838	5904.916356	15.587059	-0.053639	4.158782
266.649957	5896.922096	15.592064	-0.053693	4.156078
266.501420	5888.864543	15.597069	-0.053660	4.153345
266.473177	5880.839607	15.602074	-0.053649	4.150623
266.363826	5872.874193	15.607079	-0.053624	4.147918
266.173835	5864.834058	15.612083	-0.053583	4.145186
266.294450	5856.929207	15.617088	-0.053601	4.142501
266.032376	5848.877393	15.622093	-0.053547	4.139760
266.121455	5840.948208	15.627098	-0.053558	4.137063
266.050866	5832.888564	15.632103	-0.053540	4.134317
266.030498	5824.859117	15.637107	-0.053531	4.131581
266.178604	5816.862034	15.642112	-0.053554	4.128856
266.078308	5808.854260	15.647117	-0.053530	4.126123
266.018911	5800.905236	15.652122	-0.053514	4.123408
265.987962	5792.897427	15.657127	-0.053503	4.120672
265.845334	5784.948269	15.662131	-0.053471	4.117953
265.703390	5776.908610	15.667136	-0.053440	4.115201
265.639171	5768.847867	15.672141	-0.053422	4.112441
265.695835	5760.830976	15.677146	-0.053428	4.109695
265.864140	5752.863582	15.682151	-0.053454	4.106966
265.672759	5744.846459	15.687155	-0.053413	4.104214
265.505631	5736.958469	15.692160	-0.053377	4.101505
265.391998	5728.913849	15.697165	-0.053351	4.098740
265.429928	5720.942578	15.702170	-0.053353	4.096001
265.263466	5712.938965	15.707175	-0.053317	4.093246
265.313987	5704.880906	15.712179	-0.053321	4.090473
265.165303	5696.902942	15.717184	-0.053288	4.087724
265.030946	5688.903606	15.722189	-0.053258	4.084965
264.988954	5680.959575	15.727194	-0.053245	4.082225
264.952883	5672.932951	15.732199	-0.053233	4.079454
264.868188	5664.929056	15.737203	-0.053212	4.076689
264.952396	5656.939388	15.742208	-0.053223	4.073929
264.961946	5648.865080	15.747213	-0.053220	4.071137
264.912057	5640.916807	15.752218	-0.053205	4.068386
264.743077	5632.921879	15.757223	-0.053169	4.065616
264.758630	5624.921523	15.762227	-0.053166	4.062844
264.730296	5616.952687	15.767232	-0.053156	4.060080
264.506310	5608.969286	15.772237	-0.053109	4.057307
264.551720	5600.964373	15.777242	-0.053113	4.054528
264.694911	5592.911564	15.782247	-0.053134	4.051732
264.493572	5584.940257	15.787251	-0.053092	4.048957
264.535370	5576.934036	15.792256	-0.053094	4.046172
264.586585	5568.954442	15.797261	-0.053099	4.043394
264.505654	5560.923088	15.802266	-0.053078	4.040595
264.340084	5552.971575	15.807271	-0.053043	4.037820
264.287024	5544.903725	15.812275	-0.053027	4.035004
264.359528	5536.830007	15.817280	-0.053036	4.032186
264.263712	5528.852081	15.822285	-0.053013	4.029397
264.257444	5520.866111	15.827290	-0.053007	4.026605
264.270049	5512.907187	15.832295	-0.053004	4.023821
263.891617	5504.903647	15.837299	-0.052928	4.021013
263.960512	5496.940087	15.842304	-0.052936	4.018224
263.922249	5488.888748	15.847309	-0.052924	4.015400
264.004421	5480.889463	15.852314	-0.052934	4.012595
263.896120	5472.878264	15.857319	-0.052909	4.009780
263.831866	5464.894798	15.862323	-0.052892	4.006974
263.906899	5456.914388	15.867328	-0.052900	4.004169
263.598211	5448.909472	15.872333	-0.052838	4.001348
263.641858	5440.951445	15.877338	-0.052841	3.998546
263.511647	5432.897781	15.882343	-0.052812	3.995707
263.495591	5424.886398	15.887347	-0.052803	3.992882
263.557041	5416.871911	15.892352	-0.052810	3.990055
263.697440	5408.898412	15.897357	-0.052831	3.987241
263.513881	5400.892174	15.902362	-0.052791	3.984409
263.369604	5392.949941	15.907367	-0.052760	3.981599
263.309751	5384.899280	15.912371	-0.052743	3.978749
263.579253	5376.941539	15.917376	-0.052788	3.975935
263.296472	5368.915258	15.922381	-0.052731	3.973087
263.340296	5360.854222	15.927386	-0.052734	3.970229
263.240995	5352.943703	15.932391	-0.052710	3.967420
263.072671	5344.926054	15.937395	-0.052674	3.964570
263.188841	5337.003659	15.942400	-0.052690	3.961756
263.159433	5328.967336	15.947405	-0.052679	3.958898
263.283648	5320.947114	15.952410	-0.052697	3.956045
263.056919	5312.946656	15.957415	-0.052650	3.953192
262.784203	5304.896477	15.962419	-0.052594	3.950318
262.868949	5296.940175	15.967424	-0.052605	3.947482
262.828759	5288.922992	15.972429	-0.052592	3.944620
262.760145	5280.995154	15.977434	-0.052574	3.941787
262.777129	5273.005169	15.982439	-0.052573	3.938931
262.545414	5264.962402	15.987443	-0.052524	3.936050
262.713095	5256.963670	15.992448	-0.052550	3.933190
262.501777	5248.946581	15.997453	-0.052506	3.930314
262.557047	5240.991111	16.002458	-0.052511	3.927463
262.391510	5232.985327	16.007463	-0.052475	3.924588
262.476272	5225.009581	16.012467	-0.052486	3.921726
262.575749	5217.013704	16.017472	-0.052499	3.918855
262.347834	5208.985335	16.022477	-0.052452	3.915965
262.443098	5200.980605	16.027482	-0.052464	3.913086
262.350952	5192.972106	16.032487	-0.052442	3.910201
262.157949	5184.969470	16.037491	-0.052401	3.907313
262.137600	5176.994361	16.042496	-0.052392	3.904437
262.042847	5168.982238	16.047501	-0.052369	3.901544
261.980500	5160.985682	16.052506	-0.052353	3.898655
261.915810	5153.021975	16.057511	-0.052335	3.895775
261.869276	5144.953672	16.062515	-0.052322	3.892856
262.077359	5136.961043	16.067520	-0.052355	3.889967
261.859300	5128.991236	16.072525	-0.052310	3.887076
261.841830	5120.972231	16.077530	-0.052301	3.884169
261.899517	5112.992303	16.082535	-0.052307	3.881275
262.017623	5105.018573	16.087539	-0.052324	3.878383
261.982643	5097.032190	16.092544	-0.052312	3.875481
261.897885	5088.784070	16.097549	-0.052291	3.872480
261.871998	5080.819718	16.102554	-0.052281	3.869582
261.642964	5072.939030	16.107559	-0.052233	3.866707
261.377592	5064.938647	16.112563	-0.052179	3.863787
261.338678	5056.953667	16.117568	-0.052167	3.860874
261.332190	5048.978118	16.122573	-0.052160	3.857963
261.226643	5040.966109	16.127578	-0.052135	3.855035
261.322603	5032.956984	16.132583	-0.052148	3.852109
261.301441	5024.952611	16.137587	-0.052139	3.849181
261.174851	5017.009556	16.142592	-0.052110	3.846270
261.009411	5009.021038	16.147597	-0.052075	3.843340
261.160975	5001.016127	16.152602	-0.052098	3.840408
261.050999	4993.049585	16.157607	-0.052072	3.837483
260.931487	4985.008111	16.162611	-0.052045	3.834528
260.888699	4977.051849	16.167616	-0.052032	3.831603
261.020380	4968.994357	16.172621	-0.052051	3.828642
260.752950	4961.028161	16.177626	-0.051996	3.825705
260.874250	4953.054816	16.182631	-0.052014	3.822771
260.948246	4944.996243	16.187635	-0.052022	3.819802
260.706602	4937.103058	16.192640	-0.051972	3.816885
260.655241	4929.043753	16.197645	-0.051957	3.813908
260.735626	4921.016197	16.202650	-0.051967	3.810944
260.756766	4913.051419	16.207655	-0.051966	3.807999
260.571498	4905.061639	16.212659	-0.051927	3.805039
260.576817	4897.126173	16.217664	-0.051922	3.802100
260.532022	4889.107121	16.222669	-0.051909	3.799127
260.480896	4881.093057	16.227674	-0.051894	3.796153
260.462217	4873.082572	16.232679	-0.051886	3.793179
260.299321	4865.003642	16.237683	-0.051850	3.790174
260.287437	4857.087704	16.242688	-0.051843	3.787231
260.209515	4849.019943	16.247693	-0.051823	3.784227
260.187273	4841.084402	16.252698	-0.051814	3.781271
259.998980	4833.112988	16.257703	-0.051774	3.778296
259.993181	4825.090253	16.262707	-0.051768	3.775304
259.942327	4817.103324	16.267712	-0.051753	3.772321
259.797418	4809.049834	16.272717	-0.051721	3.769310
259.833278	4801.071311	16.277722	-0.051723	3.766328
259.669328	4793.121125	16.282727	-0.051687	3.763349
259.744880	4785.089520	16.287731	-0.051696	3.760343
259.793908	4777.120876	16.292736	-0.051700	3.757358
259.731178	4769.091284	16.297741	-0.051683	3.754345
259.667331	4761.096507	16.302746	-0.051666	3.751343
259.635386	4753.081293	16.307751	-0.051655	3.748331
259.475649	4745.080377	16.312755	-0.051620	3.745319
259.446375	4737.117759	16.317760	-0.051610	3.742322
259.550181	4729.105261	16.322765	-0.051624	3.739307
259.451329	4721.134087	16.327770	-0.051600	3.736301
259.299332	4713.114763	16.332775	-0.051567	3.733272
259.270554	4705.085250	16.337779	-0.051556	3.730241
259.555093	4697.135222	16.342784	-0.051604	3.727244
259.183399	4689.122828	16.347789	-0.051530	3.724205
259.210186	4681.176205	16.352794	-0.051530	3.721199
259.192424	4673.210793	16.357799	-0.051522	3.718182
259.127961	4665.174950	16.362803	-0.051504	3.715135
259.178652	4657.098118	16.367808	-0.051509	3.712072
259.064354	4649.086112	16.372813	-0.051482	3.709027
259.050866	4641.104693	16.377818	-0.051475	3.705994
258.944185	4633.147277	16.382823	-0.051450	3.702966
259.175708	4625.127141	16.387827	-0.051488	3.699919
259.060710	4617.210398	16.392832	-0.051461	3.696900
258.556099	4609.209114	16.397837	-0.051362	3.693838
258.582367	4601.171286	16.402842	-0.051362	3.690772
258.641299	4593.202570	16.407847	-0.051368	3.687730
258.489410	4585.189647	16.412851	-0.051334	3.684664
258.477126	4577.246134	16.417856	-0.051327	3.681625
258.561121	4569.212387	16.422861	-0.051337	3.678552
258.566125	4561.232060	16.427866	-0.051333	3.675495
258.581569	4553.217809	16.432871	-0.051331	3.672422
258.296503	4545.208200	16.437875	-0.051273	3.669341
258.217628	4537.240513	16.442880	-0.051253	3.666279
258.125839	4529.204887	16.447885	-0.051231	3.663187
258.308134	4521.192666	16.452890	-0.051260	3.660109
258.192023	4513.257340	16.457895	-0.051233	3.657051
258.039940	4505.232339	16.462899	-0.051200	3.653954
257.941842	4497.247794	16.467904	-0.051176	3.650872
257.948410	4489.254887	16.472909	-0.051172	3.647786
257.964629	4481.213979	16.477914	-0.051170	3.644680
257.968871	4473.256594	16.482919	-0.051166	3.641603
258.061583	4465.247501	16.487923	-0.051178	3.638505
258.033467	4457.276006	16.492928	-0.051168	3.635417
257.617779	4449.265421	16.497933	-0.051085	3.632300
257.879968	4441.233814	16.502938	-0.051129	3.629190
257.853318	4433.232903	16.507943	-0.051119	3.626082
257.626168	4425.285644	16.512947	-0.051071	3.622987
257.495818	4417.286434	16.517952	-0.051042	3.619872
257.611016	4409.327601	16.522957	-0.051058	3.616776
257.457331	4401.281367	16.527962	-0.051025	3.613636
257.412015	4393.291432	16.532967	-0.051011	3.610519
257.345228	4385.305933	16.537971	-0.050993	3.607399
257.280019	4377.318479	16.542976	-0.050976	3.604277
257.118923	4369.346337	16.547981	-0.050941	3.601155
257.052396	4361.376098	16.552986	-0.050924	3.598033
257.158158	4353.358379	16.557991	-0.050938	3.594896
257.301169	4345.327463	16.562995	-0.050960	3.591751
257.267033	4337.332048	16.568000	-0.050948	3.588612
257.018826	4329.330343	16.573005	-0.050897	3.585462
257.226138	4321.363480	16.578010	-0.050930	3.582336
256.940070	4313.385790	16.583015	-0.050872	3.579189
256.798541	4305.414348	16.588019	-0.050841	3.576046
257.008449	4297.394512	16.593024	-0.050875	3.572891
256.627955	4289.358780	16.598029	-0.050799	3.569710
256.582914	4281.395332	16.603034	-0.050785	3.566564
256.652230	4273.416395	16.608039	-0.050793	3.563413
256.603323	4265.397109	16.613043	-0.050779	3.560239
256.521128	4257.464683	16.618048	-0.050758	3.557097
256.456140	4249.376609	16.623053	-0.050741	3.553890
256.431208	4241.318887	16.628058	-0.050731	3.550693
256.337278	4233.371003	16.633063	-0.050709	3.547535
256.261010	4225.347259	16.638067	-0.050689	3.544345
256.423519	4217.404086	16.643072	-0.050714	3.541191
256.251925	4209.422216	16.648077	-0.050677	3.538008
256.158405	4201.409675	16.653082	-0.050655	3.534813
256.066388	4193.431703	16.658087	-0.050633	3.531629
255.952176	4185.410254	16.663091	-0.050606	3.528424
256.099671	4177.430379	16.668096	-0.050629	3.525241
256.076801	4169.479853	16.673101	-0.050619	3.522061
256.206232	4161.458740	16.678106	-0.050638	3.518854
255.787403	4153.544838	16.683111	-0.050555	3.515672
255.779458	4145.461556	16.688115	-0.050549	3.512430
255.877645	4137.474861	16.693120	-0.050562	3.509228
255.864246	4129.445668	16.698125	-0.050554	3.506002
255.691057	4121.492763	16.703130	-0.050517	3.502800
255.576841	4113.502370	16.708135	-0.050490	3.499580
255.549433	4105.538274	16.713139	-0.050480	3.496372
255.643702	4097.533426	16.718144	-0.050493	3.493147
255.486961	4089.499658	16.723149	-0.050458	3.489900
255.598206	4081.562379	16.728154	-0.050474	3.486698
255.539982	4073.577590	16.733159	-0.050458	3.483468
255.410543	4065.557976	16.738163	-0.050429	3.480218
255.337765	4057.614682	16.743168	-0.050410	3.476999
255.163876	4049.585099	16.748173	-0.050373	3.473738
255.157520	4041.556915	16.753178	-0.050366	3.470480
255.075461	4033.570659	16.758183	-0.050346	3.467233
255.054996	4025.561741	16.763187	-0.050337	3.463976
255.142129	4017.589435	16.768192	-0.050348	3.460735
254.997411	4009.623786	16.773197	-0.050316	3.457485
254.964926	4001.613157	16.778202	-0.050305	3.454218
255.147382	3993.599889	16.783207	-0.050334	3.450954
254.651549	3985.605500	16.788211	-0.050236	3.447672
254.874779	3977.619408	16.793216	-0.050273	3.444414
254.693608	3969.634335	16.798221	-0.050234	3.441140
254.586343	3961.656339	16.803226	-0.050209	3.437868
254.484494	3953.665770	16.808231	-0.050185	3.434588
254.525231	3945.633350	16.813235	-0.050187	3.431292
254.631792	3937.634442	16.818240	-0.050202	3.428010
254.552548	3929.614987	16.823245	-0.050182	3.424709
254.662081	3921.665262	16.828250	-0.050197	3.421440
254.635814	3913.712205	16.833255	-0.050187	3.418162
254.303048	3905.707878	16.838259	-0.050120	3.414850
254.348847	3897.703874	16.843264	-0.050124	3.411547
254.295414	3889.697636	16.848269	-0.050109	3.408237
254.261402	3881.689307	16.853274	-0.050097	3.404923
254.083425	3873.764744	16.858279	-0.050059	3.401636
254.040094	3865.761492	16.863283	-0.050046	3.398318
254.074421	3857.794241	16.868288	-0.050047	3.395014
253.873980	3849.678416	16.873293	-0.050005	3.391637
254.010832	3841.685293	16.878298	-0.050025	3.388319
253.966723	3833.732308	16.883303	-0.050012	3.385008
253.642882	3825.760353	16.888307	-0.049946	3.381677
253.762375	3817.801865	16.893312	-0.049963	3.378363
253.738446	3809.824316	16.898317	-0.049954	3.375033
253.673951	3801.782629	16.903322	-0.049937	3.371672
253.610063	3793.814616	16.908327	-0.049920	3.368338
253.539851	3785.796912	16.913331	-0.049902	3.364979
253.532892	3777.843695	16.918336	-0.049895	3.361647
253.323431	3769.865011	16.923341	-0.049851	3.358293
253.525264	3761.831816	16.928346	-0.049884	3.354928
253.473190	3753.841664	16.933351	-0.049869	3.351569
253.496343	3745.810823	16.938355	-0.049868	3.348191
253.300126	3737.865462	16.943360	-0.049826	3.344838
253.168410	3729.904845	16.948365	-0.049797	3.341478
253.108497	3721.931316	16.953370	-0.049780	3.338112
252.963398	3713.924469	16.958375	-0.049748	3.334725
252.899642	3705.881141	16.963379	-0.049731	3.331322
253.027057	3697.897292	16.968384	-0.049750	3.327947
252.944121	3689.907387	16.973389	-0.049729	3.324559
252.922939	3681.953393	16.978394	-0.049720	3.321186
253.006608	3673.982893	16.983399	-0.049731	3.317805
252.789431	3665.963135	16.988403	-0.049685	3.314389
252.828607	3657.935106	16.993408	-0.049687	3.310975
252.775031	3649.962344	16.998413	-0.049672	3.307578
252.644671	3641.973832	17.003418	-0.049643	3.304168
252.636497	3634.015736	17.008423	-0.049636	3.300772
252.619502	3626.018407	17.013427	-0.049628	3.297355
252.666620	3618.019307	17.018432	-0.049632	3.293937
252.300459	3610.020078	17.023437	-0.049558	3.290499
252.367584	3602.023512	17.028442	-0.049566	3.287075
252.501174	3594.064227	17.033447	-0.049586	3.283666
252.345701	3586.064918	17.038451	-0.049552	3.280225
252.419983	3578.111529	17.043456	-0.049560	3.276809
252.382491	3570.072032	17.048461	-0.049548	3.273349
252.410509	3562.058333	17.053466	-0.049548	3.269898
252.471001	3554.070411	17.058471	-0.049554	3.266456
252.265273	3546.095474	17.063475	-0.049511	3.263005
252.238789	3538.129418	17.068480	-0.049501	3.259562
252.159844	3530.159254	17.073485	-0.049481	3.256111
251.982050	3522.152548	17.078490	-0.049443	3.252637
252.155276	3514.133942	17.083495	-0.049470	3.249168
251.825461	3506.169864	17.088499	-0.049404	3.245699
251.868873	3498.203932	17.093504	-0.049407	3.242240
251.795096	3490.202008	17.098509	-0.049388	3.238757
251.864861	3482.206977	17.103514	-0.049396	3.235279
251.585346	3474.190468	17.108519	-0.049338	3.231774
251.522115	3466.162073	17.113523	-0.049322	3.228269
251.684674	3458.182224	17.118528	-0.049347	3.224790
251.477403	3450.228853	17.123533	-0.049303	3.221304
251.260973	3442.250121	17.128538	-0.049258	3.217803
251.264701	3434.252523	17.133543	-0.049253	3.214298
251.187472	3426.233520	17.138547	-0.049234	3.210777
251.139569	3418.286683	17.143552	-0.049220	3.207285
250.995800	3410.289393	17.148557	-0.049188	3.203763
251.289169	3402.278993	17.153562	-0.049237	3.200250
251.208764	3394.344348	17.158567	-0.049217	3.196750
251.048285	3386.330501	17.163571	-0.049182	3.193209
251.016392	3378.315577	17.168576	-0.049171	3.189668
250.817169	3370.345910	17.173581	-0.049129	3.186136
250.880320	3362.346850	17.178586	-0.049136	3.182599
250.850292	3354.390177	17.183591	-0.049125	3.179072
250.684482	3346.387778	17.188595	-0.049089	3.175516
250.724453	3338.402155	17.193600	-0.049091	3.171971
250.603074	3330.384752	17.198605	-0.049064	3.168402
250.557472	3322.394411	17.203610	-0.049050	3.164844
250.475870	3314.464864	17.208615	-0.049030	3.161307
250.605022	3306.433681	17.213619	-0.049049	3.157730
250.637503	3298.462098	17.218624	-0.049050	3.154172
250.255343	3290.460768	17.223629	-0.048973	3.150578
250.267750	3282.461166	17.228634	-0.048970	3.146998
250.407902	3274.483317	17.233639	-0.048991	3.143429
250.327410	3266.483781	17.238643	-0.048971	3.139837
250.056271	3258.566929	17.243648	-0.048916	3.136270
250.248742	3250.513970	17.248653	-0.048947	3.132657
250.226276	3242.530078	17.253658	-0.048937	3.129062
250.090082	3234.561691	17.258663	-0.048907	3.125465
249.928102	3226.602320	17.263667	-0.048872	3.121867
250.129361	3218.613650	17.268672	-0.048904	3.118267
250.085317	3210.612102	17.273677	-0.048891	3.114646
249.980216	3202.614898	17.278682	-0.048866	3.111021
249.899750	3194.645279	17.283687	-0.048846	3.107404
249.921147	3186.637050	17.288691	-0.048845	3.103771
249.843260	3178.663864	17.293696	-0.048825	3.100145
249.716216	3170.700836	17.298701	-0.048796	3.096517
249.578808	3162.690009	17.303706	-0.048766	3.092862
249.711939	3154.682168	17.308711	-0.048785	3.089217
249.349523	3146.713598	17.313715	-0.048713	3.085563
249.448034	3138.761580	17.318720	-0.048726	3.081933
249.298540	3130.768169	17.323725	-0.048693	3.078268
249.255029	3122.771620	17.328730	-0.048680	3.074603
249.204713	3114.698250	17.333735	-0.048665	3.070897
249.195259	3106.716799	17.338739	-0.048658	3.067231
249.201942	3098.765652	17.343744	-0.048655	3.063576
249.102572	3090.792754	17.348749	-0.048631	3.059901
249.078785	3082.849544	17.353754	-0.048621	3.056239
249.087189	3074.840911	17.358759	-0.048618	3.052543
248.849320	3066.834739	17.363763	-0.048569	3.048833
248.836695	3058.861229	17.368768	-0.048561	3.045144
248.858158	3050.901300	17.373773	-0.048560	3.041459
248.797544	3042.925808	17.378778	-0.048544	3.037758
248.713981	3034.950336	17.383783	-0.048523	3.034051
248.782495	3026.908548	17.388787	-0.048531	3.030316
248.782222	3018.938727	17.393792	-0.048525	3.026607
248.462088	3010.993071	17.398797	-0.048461	3.022889
248.464618	3003.001126	17.403802	-0.048456	3.019160
248.622141	2995.030319	17.408807	-0.048480	3.015444
248.336149	2987.030750	17.413811	-0.048422	3.011689
248.451276	2979.024754	17.418816	-0.048438	3.007945
248.434477	2971.031151	17.423821	-0.048430	3.004196
248.157537	2963.087421	17.428826	-0.048373	3.000453
248.041251	2955.149496	17.433831	-0.048347	2.996716
248.099104	2947.099805	17.438835	-0.048352	2.992931
248.054916	2939.102140	17.443840	-0.048339	2.989160
247.991617	2931.115286	17.448845	-0.048322	2.985388
247.925806	2923.142788	17.453850	-0.048305	2.981618
247.920825	2915.185836	17.458855	-0.048299	2.977854
247.828149	2907.163940	17.463859	-0.048276	2.974050
247.698754	2899.199025	17.468864	-0.048247	2.970266
247.805570	2891.217193	17.473869	-0.048262	2.966481
247.871925	2883.230781	17.478874	-0.048269	2.962687
247.904389	2875.256879	17.483879	-0.048270	2.958893
247.760762	2867.278670	17.488883	-0.048238	2.955082
247.759376	2859.260266	17.493888	-0.048233	2.951255
247.602731	2851.296375	17.498893	-0.048199	2.947441
247.583540	2843.312426	17.503898	-0.048190	2.943619
247.503929	2835.360350	17.508903	-0.048170	2.939805
247.256020	2827.393261	17.513907	-0.048119	2.935969
247.129422	2819.400200	17.518912	-0.048090	2.932123
247.204803	2811.395138	17.523917	-0.048099	2.928276
247.125397	2803.436807	17.528922	-0.048079	2.924438
247.228671	2795.449026	17.533927	-0.048093	2.920591
247.090264	2787.469003	17.538931	-0.048062	2.916730
247.248921	2779.421361	17.543936	-0.048087	2.912846
246.977944	2771.428169	17.548941	-0.048031	2.908961
246.925177	2763.448898	17.553946	-0.048016	2.905089
246.843461	2755.514317	17.558951	-0.047996	2.901232
246.794799	2747.522524	17.563955	-0.047982	2.897344
246.652339	2739.555028	17.568960	-0.047950	2.893458
246.675162	2731.543585	17.573965	-0.047949	2.889553
246.507598	2723.585748	17.578970	-0.047913	2.885660
246.429308	2715.637785	17.583975	-0.047893	2.881770
246.476397	2707.647159	17.588979	-0.047897	2.877861
246.556722	2699.643936	17.593984	-0.047907	2.873943
246.419790	2691.661803	17.598989	-0.047876	2.870018
246.365794	2683.666809	17.603994	-0.047861	2.866085
246.509499	2675.699384	17.608999	-0.047883	2.862172
246.202616	2667.747658	17.614003	-0.047821	2.858236
246.308247	2659.760145	17.619008	-0.047835	2.854300
246.147332	2651.766200	17.624013	-0.047800	2.850340
246.223414	2643.800270	17.629018	-0.047809	2.846402
246.077388	2635.841408	17.634023	-0.047777	2.842449
245.893764	2627.875941	17.639027	-0.047738	2.838486
245.962751	2619.878678	17.644032	-0.047745	2.834516
245.903061	2611.863913	17.649037	-0.047729	2.830523
245.734389	2603.892892	17.654042	-0.047693	2.826541
246.017655	2595.924930	17.659047	-0.047740	2.822581
245.765366	2587.959095	17.664051	-0.047688	2.818585
245.820280	2579.970882	17.669056	-0.047693	2.814590
245.744976	2571.978365	17.674061	-0.047674	2.810580
245.721602	2563.991971	17.679066	-0.047665	2.806570
245.468804	2556.059457	17.684071	-0.047612	2.802568
245.311422	2548.081584	17.689075	-0.047578	2.798543
245.398070	2540.105755	17.694080	-0.047589	2.794528
245.211703	2532.085680	17.699085	-0.047549	2.790468
245.224942	2524.117888	17.704090	-0.047547	2.786441
245.309916	2516.156389	17.709095	-0.047557	2.782415
245.160001	2508.170821	17.714099	-0.047524	2.778358
245.190795	2500.202446	17.719104	-0.047525	2.774313
245.109040	2492.204155	17.724109	-0.047505	2.770241
245.075649	2484.227964	17.729114	-0.047493	2.766177
245.073932	2476.296519	17.734119	-0.047488	2.762132
244.809875	2468.332217	17.739123	-0.047434	2.758049
244.954294	2460.318023	17.744128	-0.047455	2.753958
244.941839	2452.258532	17.749133	-0.047448	2.749828
244.581366	2444.333499	17.754138	-0.047376	2.745741
244.618822	2436.385200	17.759143	-0.047378	2.741659
244.582084	2428.391981	17.764147	-0.047366	2.737544
244.568803	2420.418929	17.769152	-0.047358	2.733434
244.642520	2412.410116	17.774157	-0.047367	2.729305
244.329826	2404.464561	17.779162	-0.047303	2.725178
244.475273	2396.508218	17.784167	-0.047325	2.721068
244.460327	2388.553984	17.789171	-0.047318	2.716943
244.518428	2380.538264	17.794176	-0.047323	2.712784
244.383527	2372.559602	17.799181	-0.047293	2.708626
244.196011	2364.613320	17.804186	-0.047253	2.704476
244.225083	2356.650457	17.809191	-0.047253	2.700323
244.109091	2348.680773	17.814195	-0.047227	2.696152
244.040124	2340.704136	17.819200	-0.047209	2.691974
243.825321	2332.724707	17.824205	-0.047164	2.687778
243.911259	2324.734740	17.829210	-0.047175	2.683589
243.886583	2316.806130	17.834215	-0.047165	2.679419
243.595215	2308.852759	17.839219	-0.047106	2.675213
243.741655	2300.822449	17.844224	-0.047128	2.670987
243.627368	2292.837521	17.849229	-0.047101	2.666761
243.495840	2284.883323	17.854234	-0.047072	2.662544
243.692045	2276.893735	17.859239	-0.047103	2.658323
243.637642	2268.910193	17.864243	-0.047088	2.654082
243.474398	2260.938038	17.869248	-0.047052	2.649833
243.469466	2252.974665	17.874253	-0.047046	2.645593
243.319766	2245.047319	17.879258	-0.047013	2.641355
243.302999	2237.089634	17.884263	-0.047005	2.637103
242.909706	2229.117812	17.889267	-0.046927	2.632812
242.992686	2221.127180	17.894272	-0.046937	2.628535
243.136177	2213.108640	17.899277	-0.046959	2.624240
243.119816	2205.139376	17.904282	-0.046951	2.619954
243.197944	2197.202772	17.909287	-0.046960	2.615685
243.039856	2189.216916	17.914291	-0.046926	2.611366
242.956688	2181.255866	17.919296	-0.046905	2.607059
242.871938	2173.304755	17.924301	-0.046884	2.602750
242.836098	2165.347260	17.929306	-0.046872	2.598433
242.735886	2157.345243	17.934311	-0.046849	2.594081
242.583751	2149.208066	17.939315	-0.046815	2.589645
242.585731	2141.268335	17.944320	-0.046810	2.585318
242.541249	2133.339696	17.949325	-0.046797	2.580988
242.510298	2125.384750	17.954330	-0.046786	2.576637
242.485191	2117.451921	17.959335	-0.046776	2.572290
242.399234	2109.479309	17.964339	-0.046755	2.567911
242.381187	2101.527697	17.969344	-0.046747	2.563540
242.268607	2093.586544	17.974349	-0.046721	2.559161
242.186845	2085.612731	17.979354	-0.046701	2.554758
242.410828	2077.613789	17.984359	-0.046737	2.550356
242.237020	2069.650675	17.989363	-0.046700	2.545938
242.311860	2061.702607	17.994368	-0.046709	2.541537
242.218826	2053.746026	17.999373	-0.046686	2.537113
242.053547	2045.778632	18.004378	-0.046650	2.532670
241.801816	2037.848359	18.009383	-0.046598	2.528233
241.741882	2029.873047	18.014387	-0.046582	2.523777
241.706009	2021.917424	18.019392	-0.046570	2.519326
241.473028	2013.966844	18.024397	-0.046522	2.514856
241.477743	2005.934218	18.029402	-0.046518	2.510349
241.619679	1997.963320	18.034407	-0.046539	2.505878
241.481880	1990.004283	18.039411	-0.046508	2.501386
241.397000	1982.068015	18.044416	-0.046487	2.496902
241.313301	1974.093746	18.049421	-0.046467	2.492389
241.225994	1966.125066	18.054426	-0.046445	2.487871
241.243282	1958.167836	18.059431	-0.046443	2.483358
241.183076	1950.210661	18.064435	-0.046427	2.478832
241.241692	1942.242508	18.069440	-0.046433	2.474299
241.159626	1934.265620	18.074445	-0.046413	2.469744
240.987873	1926.306972	18.079450	-0.046375	2.465183
240.985420	1918.368615	18.084455	-0.046370	2.460638
240.828897	1910.399758	18.089459	-0.046336	2.456056
240.712294	1902.440378	18.094464	-0.046309	2.451473
240.859678	1894.454636	18.099469	-0.046331	2.446887
240.539915	1886.530374	18.104474	-0.046267	2.442292
240.487324	1878.590479	18.109479	-0.046252	2.437700
240.464160	1870.574163	18.114483	-0.046242	2.433057
240.493822	1862.569699	18.119488	-0.046243	2.428416
240.288017	1854.624155	18.124493	-0.046199	2.423782
240.141812	1846.679099	18.129498	-0.046167	2.419144
240.384729	1838.704608	18.134503	-0.046207	2.414510
240.522546	1830.697815	18.139507	-0.046228	2.409841
240.255008	1822.792404	18.144512	-0.046173	2.405190
240.325442	1814.830998	18.149517	-0.046181	2.400523
240.226380	1806.904638	18.154522	-0.046157	2.395855
239.934782	1798.972302	18.159527	-0.046098	2.391159
239.849869	1790.978234	18.164531	-0.046077	2.386434
239.911966	1783.025763	18.169536	-0.046084	2.381735
239.941830	1775.068510	18.174541	-0.046084	2.377022
239.677515	1767.125444	18.179546	-0.046030	2.372284
239.700039	1759.147092	18.184551	-0.046029	2.367539
239.596248	1751.202201	18.189555	-0.046004	2.362794
239.749478	1743.245541	18.194560	-0.046028	2.358053
239.658206	1735.279353	18.199565	-0.046006	2.353277
239.659499	1727.281283	18.204570	-0.046001	2.348480
239.498579	1719.363748	18.209575	-0.045966	2.343708
239.261148	1711.426957	18.214579	-0.045917	2.338909
239.385136	1703.464096	18.219584	-0.045935	2.334113
239.211601	1695.505272	18.224589	-0.045897	2.329286
238.983887	1687.569385	18.229594	-0.045850	2.324458
239.090497	1679.623894	18.234599	-0.045864	2.319641
239.150374	1671.662240	18.239603	-0.045871	2.314801
238.969505	1663.688158	18.244608	-0.045832	2.309924
238.802631	1655.749784	18.249613	-0.045796	2.305058
238.800358	1647.797853	18.254618	-0.045790	2.300188
238.875353	1639.850385	18.259623	-0.045799	2.295317
238.812432	1631.867913	18.264627	-0.045782	2.290403
238.776824	1623.926428	18.269632	-0.045770	2.285505
238.604269	1616.017036	18.274637	-0.045733	2.280605
238.410650	1608.085330	18.279642	-0.045692	2.275679
238.541734	1600.041148	18.284647	-0.045711	2.270700
238.625866	1592.043316	18.289651	-0.045722	2.265735
238.634916	1584.127140	18.294656	-0.045719	2.260803
238.494125	1576.206781	18.299661	-0.045687	2.255845
238.461870	1568.235286	18.304666	-0.045676	2.250854
238.397944	1560.293093	18.309671	-0.045659	2.245867
238.258370	1552.369425	18.314675	-0.045628	2.240874
238.158058	1544.448623	18.319680	-0.045604	2.235875
238.155738	1536.472403	18.324685	-0.045599	2.230838
238.052949	1528.518368	18.329690	-0.045575	2.225796
238.185408	1520.582926	18.334695	-0.045594	2.220774
237.919154	1512.662581	18.339699	-0.045540	2.215715
237.899481	1504.696531	18.344704	-0.045531	2.210637
237.855032	1496.750798	18.349709	-0.045518	2.205559
237.528317	1488.859205	18.354714	-0.045452	2.200478
237.560330	1480.916551	18.359719	-0.045453	2.195385
237.305197	1472.932681	18.364723	-0.045400	2.190227
237.525932	1464.948191	18.369728	-0.045436	2.185100
237.631697	1456.997085	18.374733	-0.045450	2.179972
237.229693	1449.111503	18.379738	-0.045371	2.174828
237.158787	1441.157288	18.384743	-0.045352	2.169657
237.158279	1433.202483	18.389747	-0.045347	2.164481
237.245825	1425.269460	18.394752	-0.045358	2.159314
237.231868	1417.339760	18.399757	-0.045351	2.154127
237.128639	1409.376474	18.404762	-0.045326	2.148898
236.945737	1401.459195	18.409767	-0.045287	2.143679
237.108039	1393.493000	18.414771	-0.045312	2.138447
236.925250	1385.580952	18.419776	-0.045273	2.133205
237.004927	1377.620672	18.424781	-0.045283	2.127944
236.814982	1369.702279	18.429786	-0.045243	2.122671
236.923883	1361.775936	18.434791	-0.045258	2.117409
236.713817	1353.805253	18.439795	-0.045214	2.112073
236.561558	1345.860738	18.444800	-0.045180	2.106747
236.495687	1337.927654	18.449805	-0.045163	2.101424
236.333492	1330.007517	18.454810	-0.045128	2.096086
236.309874	1322.076023	18.459815	-0.045118	2.090740
236.133965	1314.136800	18.464819	-0.045080	2.085361
236.214317	1306.208371	18.469824	-0.045090	2.080000
236.242882	1298.277976	18.474829	-0.045090	2.074618
236.127606	1290.328586	18.479834	-0.045064	2.069196
236.136804	1282.392466	18.484839	-0.045061	2.063781
236.061664	1274.472822	18.489843	-0.045041	2.058354
236.021531	1266.558985	18.494848	-0.045029	2.052921
235.945126	1258.619067	18.499853	-0.045010	2.047451
235.864372	1250.701941	18.504858	-0.044990	2.041982
235.775529	1242.797559	18.509863	-0.044968	2.036506
235.561970	1234.859296	18.514867	-0.044923	2.030980
235.728558	1226.896053	18.519872	-0.044949	2.025459
235.540652	1219.001437	18.524877	-0.044909	2.019935
235.275207	1211.096946	18.529882	-0.044855	2.014381
235.347373	1203.141902	18.534887	-0.044863	2.008811
235.466455	1195.181059	18.539891	-0.044880	2.003227
235.178450	1187.322469	18.544896	-0.044821	1.997656
235.025301	1179.400086	18.549901	-0.044788	1.992039
235.160402	1171.420857	18.554906	-0.044808	1.986396
235.029278	1163.538158	18.559911	-0.044778	1.980777
234.873389	1155.627813	18.564915	-0.044744	1.975120
234.864493	1147.688896	18.569920	-0.044738	1.969442
234.884973	1139.763252	18.574925	-0.044736	1.963760
234.660970	1131.889662	18.579930	-0.044690	1.958073
234.633098	1123.945798	18.584935	-0.044679	1.952339
234.403649	1116.004185	18.589939	-0.044631	1.946569
234.557366	1108.072840	18.594944	-0.044655	1.940830
234.410209	1100.175074	18.599949	-0.044623	1.935066
234.407374	1092.226273	18.604954	-0.044617	1.929263
234.425190	1084.320599	18.609959	-0.044615	1.923477
234.146622	1076.445363	18.614963	-0.044558	1.917663
234.061658	1068.540653	18.619968	-0.044537	1.911831
234.272508	1060.566238	18.624973	-0.044572	1.905962
233.995383	1052.697806	18.629978	-0.044515	1.900099
233.803255	1044.834062	18.634983	-0.044474	1.894231
233.827080	1036.880751	18.639987	-0.044473	1.888303
233.851378	1028.971665	18.644992	-0.044473	1.882388
233.663424	1021.098275	18.649997	-0.044433	1.876458
233.590776	1013.155331	18.655002	-0.044414	1.870470
233.753504	1005.224445	18.660007	-0.044440	1.864499
233.630435	997.330751	18.665011	-0.044412	1.858503
233.517894	989.438232	18.670016	-0.044386	1.852491
233.571815	981.508928	18.675021	-0.044391	1.846450
233.372277	973.644132	18.680026	-0.044348	1.840409
233.334300	965.765682	18.685031	-0.044336	1.834356
233.169584	957.854602	18.690035	-0.044301	1.828243
233.263017	949.931579	18.695040	-0.044313	1.822132
233.148267	942.056230	18.700045	-0.044286	1.816011
232.876292	934.176060	18.705050	-0.044231	1.809848
233.072406	926.257636	18.710055	-0.044262	1.803690
232.979450	918.375918	18.715059	-0.044240	1.797504
232.749311	910.466486	18.720064	-0.044192	1.791259
232.702743	902.542523	18.725069	-0.044178	1.785002
232.375398	894.703300	18.730074	-0.044112	1.778757
232.430944	886.796473	18.735079	-0.044118	1.772482
232.361007	878.887226	18.740083	-0.044100	1.766168
232.430102	871.001371	18.745088	-0.044107	1.759868
232.337044	863.141184	18.750093	-0.044085	1.753545
232.123554	855.250660	18.755098	-0.044040	1.747159
232.284089	847.354927	18.760103	-0.044065	1.740793
232.113822	839.488220	18.765107	-0.044028	1.734385
231.995088	831.613553	18.770112	-0.044001	1.727954
231.980824	823.741394	18.775117	-0.043993	1.721514
231.822189	815.874458	18.780122	-0.043959	1.715035
231.849553	807.965358	18.785127	-0.043959	1.708521
231.790701	800.077881	18.790131	-0.043943	1.701989
231.743954	792.219715	18.795136	-0.043929	1.695458
231.689523	784.341823	18.800141	-0.043914	1.688884
231.543818	776.485572	18.805146	-0.043882	1.682290
231.639332	768.611647	18.810151	-0.043895	1.675687
231.405951	760.752749	18.815155	-0.043846	1.669027
231.335962	752.895977	18.820160	-0.043828	1.662364
231.318864	745.025302	18.825165	-0.043820	1.655670
231.143903	737.166998	18.830170	-0.043782	1.648937
231.191886	729.309947	18.835175	-0.043786	1.642208
230.823251	721.493852	18.840179	-0.043713	1.635430
230.964119	713.543550	18.845184	-0.043734	1.628578
230.934543	705.682623	18.850189	-0.043723	1.621750
230.739331	697.854278	18.855194	-0.043682	1.614899
230.704829	690.000804	18.860199	-0.043670	1.608020
230.686464	682.140225	18.865203	-0.043662	1.601106
230.524397	674.333088	18.870208	-0.043627	1.594190
230.558516	666.447601	18.875213	-0.043628	1.587202
230.409437	658.620095	18.880218	-0.043595	1.580208
230.366338	650.797541	18.885223	-0.043582	1.573203
230.383238	642.921437	18.890227	-0.043580	1.566128
230.229798	635.127149	18.895232	-0.043547	1.559069
230.181952	627.283854	18.900237	-0.043533	1.551949
229.992579	619.441661	18.905242	-0.043493	1.544776
229.915685	611.633952	18.910247	-0.043473	1.537618
229.798534	603.786156	18.915251	-0.043447	1.530383
229.773557	595.958178	18.920256	-0.043437	1.523147
229.659740	588.153447	18.925261	-0.043411	1.515884
229.607287	580.308729	18.930266	-0.043396	1.508558
229.480213	572.511596	18.935271	-0.043367	1.501229
229.131504	564.735878	18.940275	-0.043297	1.493851
229.249231	556.870358	18.945280	-0.043314	1.486422
229.272647	549.063604	18.950285	-0.043314	1.478998
229.029258	541.249910	18.955290	-0.043263	1.471488
229.113307	533.402835	18.960295	-0.043274	1.463959
229.051192	525.601710	18.965299	-0.043257	1.456412
228.910752	517.813307	18.970304	-0.043226	1.448826
228.877356	510.018165	18.975309	-0.043215	1.441210
228.707488	502.246829	18.980314	-0.043178	1.433555
228.575500	494.461314	18.985319	-0.043149	1.425851
228.470210	486.682920	18.990323	-0.043124	1.418117
228.445398	478.882798	18.995328	-0.043115	1.410332
228.089735	471.147833	19.000333	-0.043044	1.402514
227.821018	463.392238	19.005338	-0.042989	1.394646
227.984949	455.559297	19.010343	-0.043014	1.386727
227.690315	447.820829	19.015347	-0.042954	1.378782
227.647430	440.034556	19.020352	-0.042941	1.370784
227.902165	432.223744	19.025357	-0.042984	1.362765
227.639244	424.496431	19.030362	-0.042930	1.354696
227.525655	416.746209	19.035367	-0.042904	1.346581
227.415845	408.993959	19.040371	-0.042878	1.338415
227.525121	401.215079	19.045376	-0.042894	1.330209
227.254773	393.506202	19.050381	-0.042839	1.321960
227.088705	385.749491	19.055386	-0.042803	1.313626
227.281846	377.872055	19.060391	-0.042834	1.305173
227.105799	370.174509	19.065395	-0.042796	1.296793
226.996438	362.458788	19.070400	-0.042771	1.288351
226.842084	354.775785	19.075405	-0.042737	1.279881
226.596213	347.079998	19.080410	-0.042686	1.271324
226.509804	339.378506	19.085415	-0.042665	1.262732
226.338728	331.690263	19.090419	-0.042628	1.254080
226.329674	323.976287	19.095424	-0.042622	1.245369
226.262027	316.296399	19.100429	-0.042604	1.236625
226.302232	308.565654	19.105434	-0.042607	1.227781
226.287946	300.887114	19.110439	-0.042599	1.218922
225.962158	293.246969	19.115443	-0.042534	1.209982
225.752540	285.597277	19.120448	-0.042490	1.200987
225.670791	277.941709	19.125453	-0.042470	1.191943
225.603960	270.268066	19.130458	-0.042452	1.182811
225.662366	262.606678	19.135463	-0.042458	1.173649
225.371617	254.993107	19.140467	-0.042399	1.164400
225.263323	247.376624	19.145472	-0.042374	1.155111
225.246315	239.689730	19.150477	-0.042366	1.145680
224.988869	232.097291	19.155482	-0.042313	1.136236
224.838987	224.491496	19.160487	-0.042281	1.126720
224.952995	216.857545	19.165491	-0.042297	1.117144
224.641035	209.301128	19.170496	-0.042234	1.107490
224.471575	201.727511	19.175501	-0.042198	1.097762
224.305551	194.152991	19.180506	-0.042162	1.087945
224.261430	186.588836	19.185511	-0.042149	1.078081
224.144787	179.015145	19.190515	-0.042122	1.068096
223.889930	171.495025	19.195520	-0.042070	1.058056
223.871087	163.935584	19.200525	-0.042062	1.047922
223.558070	156.448977	19.205530	-0.041999	1.037718
223.480627	148.933027	19.210535	-0.041980	1.027430
223.113149	141.467373	19.215539	-0.041906	1.017036
222.818613	134.000152	19.220544	-0.041847	1.006551
222.536962	126.552908	19.225549	-0.041790	0.995987
222.332721	119.047561	19.230554	-0.041747	0.985246
222.102778	111.613775	19.235559	-0.041699	0.974483
221.503149	104.232708	19.240563	-0.041583	0.963582
221.053073	96.855414	19.245568	-0.041494	0.952601
220.758043	89.454459	19.250573	-0.041435	0.941497
220.374714	82.086630	19.255578	-0.041359	0.930286
219.905443	74.755609	19.260583	-0.041266	0.918972
219.467481	67.416315	19.265587	-0.041180	0.907513
218.927587	60.356364	19.270592	-0.041075	0.896318