Fri Mar 12 11:01:15 2021


Number of Points = 3618

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
1.810782	-0.018954	0.000000	-0.000011	0.733411
1.517979	0.036680	0.005005	0.000043	0.733419
1.286162	0.072619	0.010010	0.000085	0.733410
1.861581	-0.027148	0.015014	-0.000023	0.733417
2.293494	-0.106592	0.020019	-0.000104	0.733414
2.255840	-0.101725	0.025024	-0.000098	0.733412
2.180978	-0.086401	0.030029	-0.000085	0.733417
2.152240	-0.162719	0.035034	-0.000081	0.733261
1.954282	-0.218561	0.040038	-0.000045	0.733087
1.998143	-0.229247	0.045043	-0.000054	0.733083
1.717369	-0.179387	0.050048	-0.000002	0.733084
1.070712	-0.061280	0.055053	0.000117	0.733092
1.208135	-0.092003	0.060058	0.000091	0.733081
1.851890	-0.204215	0.065062	-0.000030	0.733087
1.790773	-0.198362	0.070067	-0.000019	0.733079
1.764533	-0.194879	0.075072	-0.000015	0.733078
1.876163	-0.209346	0.080077	-0.000037	0.733090
1.827550	-0.271395	0.085082	-0.000029	0.732955
1.485611	-0.303396	0.090086	0.000034	0.732777
1.560894	-0.319793	0.095091	0.000019	0.732773
1.699918	-0.348459	0.100096	-0.000007	0.732767
1.611863	-0.328086	0.105101	0.000008	0.732778
1.602573	-0.331694	0.110106	0.000009	0.732769
1.920588	-0.422309	0.115110	-0.000051	0.732705
1.764667	-0.525697	0.120115	-0.000023	0.732453
1.162353	-0.420400	0.125120	0.000088	0.732451
1.142358	-0.413833	0.130125	0.000091	0.732458
1.233264	-0.435509	0.135130	0.000074	0.732449
1.143453	-0.417649	0.140134	0.000089	0.732455
1.237717	-0.568086	0.145139	0.000071	0.732197
1.414813	-0.627394	0.150144	0.000037	0.732145
1.611217	-0.657559	0.155149	-0.000000	0.732156
1.326553	-0.613537	0.160154	0.000052	0.732145
1.406009	-0.713439	0.165158	0.000036	0.731980
1.193600	-0.753732	0.170163	0.000075	0.731831
0.920009	-0.708090	0.175168	0.000125	0.731826
1.151600	-0.746655	0.180173	0.000081	0.731833
1.336391	-0.866755	0.185178	0.000046	0.731666
1.524724	-0.974979	0.190182	0.000010	0.731523
1.464513	-0.966175	0.195187	0.000020	0.731521
1.235687	-0.953794	0.200192	0.000062	0.731467
1.114065	-1.062537	0.205197	0.000084	0.731216
1.043801	-1.058467	0.210202	0.000096	0.731201
1.066342	-1.058670	0.215206	0.000091	0.731210
1.007445	-1.176476	0.220211	0.000101	0.730963
0.889611	-1.180764	0.225216	0.000122	0.730916
0.923106	-1.183522	0.230221	0.000115	0.730924
1.106433	-1.346433	0.235226	0.000081	0.730673
0.774243	-1.330027	0.240230	0.000141	0.730591
-0.136340	-1.168447	0.245235	0.000310	0.730592
0.076349	-1.296865	0.250240	0.000270	0.730418
0.861499	-1.509844	0.255245	0.000123	0.730277
1.071474	-1.553180	0.260250	0.000083	0.730267
0.854795	-1.636793	0.265254	0.000122	0.730032
0.554127	-1.623545	0.270259	0.000177	0.729955
0.722863	-1.673811	0.275264	0.000145	0.729918
0.951503	-1.850517	0.280269	0.000102	0.729655
0.739142	-1.819373	0.285274	0.000141	0.729644
0.000878	-1.786958	0.290278	0.000277	0.729453
-0.415159	-1.778125	0.295283	0.000354	0.729328
-0.094527	-1.837978	0.300288	0.000293	0.729324
-1.121279	-1.779708	0.305293	0.000484	0.729084
-1.743839	-1.703174	0.310298	0.000599	0.729019
-1.826905	-1.686042	0.315302	0.000613	0.729025
-1.903480	-1.734170	0.320307	0.000627	0.728906
-2.601044	-1.715226	0.325312	0.000756	0.728703
-2.022341	-1.814590	0.330317	0.000647	0.728712
-2.572615	-1.726265	0.335322	0.000749	0.728695
-2.837629	-1.792294	0.340326	0.000797	0.728476
-3.372382	-1.736248	0.345331	0.000896	0.728402
-3.525903	-1.712113	0.350336	0.000923	0.728397
-3.253728	-1.755923	0.355341	0.000872	0.728408
-3.641049	-1.799335	0.360346	0.000943	0.728191
-4.645885	-1.682616	0.365350	0.001129	0.728071
-4.291223	-1.747765	0.370355	0.001063	0.728069
-4.593843	-1.698816	0.375360	0.001118	0.728061
-4.521342	-1.708213	0.380365	0.001104	0.728070
-5.013861	-1.763181	0.385370	0.001195	0.727793
-5.387882	-1.717028	0.390374	0.001263	0.727755
-5.189309	-1.755278	0.395379	0.001225	0.727751
-5.251017	-1.748043	0.400384	0.001236	0.727746
-5.307921	-1.733608	0.405389	0.001246	0.727756
-5.525979	-1.812287	0.410394	0.001286	0.727528
-6.624839	-1.662223	0.415398	0.001489	0.727441
-6.212932	-1.738966	0.420403	0.001412	0.727436
-6.419879	-1.703354	0.425408	0.001449	0.727435
-6.115215	-1.756603	0.430413	0.001392	0.727439
-6.239324	-1.736617	0.435418	0.001414	0.727436
-6.751498	-1.794439	0.440422	0.001509	0.727148
-6.933009	-1.762834	0.445427	0.001542	0.727148
-7.560169	-1.653706	0.450432	0.001657	0.727144
-6.822136	-1.785496	0.455437	0.001519	0.727145
-7.011199	-1.755509	0.460442	0.001554	0.727140
-7.321398	-1.706442	0.465446	0.001610	0.727129
-7.557525	-1.821896	0.470451	0.001654	0.726824
-7.907392	-1.761363	0.475456	0.001718	0.726822
-8.118105	-1.720278	0.480461	0.001756	0.726831
-8.194243	-1.712710	0.485466	0.001769	0.726821
-8.064103	-1.734297	0.490470	0.001744	0.726825
-8.019460	-1.743587	0.495475	0.001735	0.726824
-8.397774	-1.795780	0.500480	0.001805	0.726593
-9.186967	-1.694445	0.505485	0.001951	0.726518
-8.902216	-1.748075	0.510490	0.001897	0.726514
-8.769264	-1.770764	0.515494	0.001871	0.726517
-8.856412	-1.757914	0.520499	0.001887	0.726514
-9.081370	-1.719414	0.525504	0.001928	0.726512
-8.657489	-1.821808	0.530509	0.001848	0.726461
-10.056645	-1.707174	0.535514	0.002108	0.726201
-9.995176	-1.717620	0.540518	0.002095	0.726203
-9.949686	-1.726700	0.545523	0.002086	0.726203
-10.162739	-1.691477	0.550528	0.002125	0.726199
-9.961548	-1.726475	0.555533	0.002087	0.726202
-10.076471	-1.709279	0.560538	0.002107	0.726198
-9.837674	-1.749052	0.565542	0.002062	0.726205
-10.221874	-1.810080	0.570547	0.002132	0.725953
-10.774673	-1.727526	0.575552	0.002234	0.725924
-10.560368	-1.763540	0.580557	0.002194	0.725930
-10.668273	-1.749151	0.585562	0.002213	0.725922
-10.680519	-1.745836	0.590566	0.002214	0.725926
-10.499540	-1.775958	0.595571	0.002180	0.725932
-10.670605	-1.827330	0.600576	0.002211	0.725773
-11.871619	-1.701489	0.605581	0.002434	0.725603
-11.417502	-1.788145	0.610586	0.002348	0.725593
-11.474005	-1.776713	0.615590	0.002358	0.725598
-11.820960	-1.713735	0.620595	0.002422	0.725602
-11.970617	-1.693350	0.625600	0.002449	0.725591
-11.645850	-1.746274	0.630605	0.002387	0.725602
-11.834628	-1.753675	0.635610	0.002422	0.725524
-12.508921	-1.752750	0.640614	0.002546	0.725292
-12.188367	-1.812674	0.645619	0.002486	0.725289
-13.021098	-1.666453	0.650624	0.002640	0.725286
-12.686302	-1.722763	0.655629	0.002577	0.725294
-12.652710	-1.734478	0.660634	0.002570	0.725285
-12.916573	-1.685613	0.665638	0.002618	0.725290
-12.836574	-1.700238	0.670643	0.002602	0.725291
-12.973996	-1.809892	0.675648	0.002627	0.725030
-13.169830	-1.802873	0.680653	0.002662	0.724977
-13.918514	-1.672368	0.685658	0.002801	0.724973
-13.807389	-1.691298	0.690662	0.002779	0.724977
-13.431163	-1.759817	0.695667	0.002708	0.724975
-13.581949	-1.735911	0.700672	0.002736	0.724971
-13.545730	-1.737675	0.705677	0.002728	0.724982
-13.948957	-1.738824	0.710682	0.002802	0.724841
-14.678530	-1.698017	0.715686	0.002937	0.724668
-14.347051	-1.752307	0.720691	0.002875	0.724679
-14.897849	-1.661376	0.725696	0.002976	0.724667
-14.571802	-1.713981	0.730701	0.002915	0.724679
-14.659422	-1.703833	0.735706	0.002930	0.724670
-14.858512	-1.667338	0.740710	0.002966	0.724674
-14.572735	-1.717561	0.745715	0.002912	0.724677
-14.859862	-1.794024	0.750720	0.002965	0.724429
-15.863224	-1.665264	0.755725	0.003151	0.724333
-15.911545	-1.661113	0.760730	0.003159	0.724325
-15.592338	-1.714299	0.765734	0.003099	0.724334
-15.862658	-1.669469	0.770739	0.003148	0.724329
-16.001431	-1.648457	0.775744	0.003173	0.724324
-15.292751	-1.763167	0.780749	0.003040	0.724348
-15.614495	-1.714524	0.785754	0.003099	0.724332
-15.899314	-1.780851	0.790758	0.003152	0.724105
-16.738025	-1.687674	0.795763	0.003307	0.723997
-16.660780	-1.699540	0.800768	0.003292	0.724002
-16.561118	-1.713443	0.805773	0.003272	0.724011
-16.989802	-1.646633	0.810778	0.003351	0.723994
-16.721200	-1.689818	0.815782	0.003300	0.724005
-16.774909	-1.682314	0.820787	0.003310	0.724002
-17.094708	-1.632697	0.825792	0.003368	0.723990
-16.712601	-1.776146	0.830797	0.003296	0.723843
-17.803787	-1.676995	0.835802	0.003498	0.723659
-17.709196	-1.692468	0.840806	0.003480	0.723663
-17.791250	-1.677886	0.845811	0.003494	0.723665
-17.821062	-1.676548	0.850816	0.003499	0.723658
-17.742360	-1.687201	0.855821	0.003484	0.723667
-18.013978	-1.647711	0.860826	0.003533	0.723651
-17.764206	-1.688981	0.865830	0.003486	0.723659
-17.686224	-1.758774	0.870835	0.003471	0.723551
-18.818212	-1.659122	0.875840	0.003680	0.723353
-18.426635	-1.723691	0.880845	0.003607	0.723364
-18.706732	-1.680219	0.885850	0.003658	0.723353
-19.023977	-1.624996	0.890854	0.003716	0.723353
-18.523667	-1.711313	0.895859	0.003622	0.723360
-18.650227	-1.693505	0.900864	0.003645	0.723352
-18.594513	-1.699072	0.905869	0.003634	0.723362
-18.912969	-1.746902	0.910874	0.003692	0.723159
-19.800728	-1.664527	0.915878	0.003857	0.723012
-19.407695	-1.732504	0.920883	0.003783	0.723018
-19.740884	-1.678500	0.925888	0.003844	0.723009
-19.592435	-1.702571	0.930893	0.003815	0.723015
-19.329295	-1.753986	0.935898	0.003765	0.723008
-19.618669	-1.702372	0.940902	0.003818	0.723009
-19.687059	-1.692132	0.945907	0.003830	0.723007
-20.212584	-1.759608	0.950912	0.003927	0.722693
-20.197546	-1.758614	0.955917	0.003924	0.722702
-20.960221	-1.627778	0.960922	0.004065	0.722694
-20.734823	-1.668933	0.965926	0.004022	0.722693
-20.504798	-1.709121	0.970931	0.003978	0.722696
-21.092719	-1.606695	0.975936	0.004087	0.722694
-20.397574	-1.726836	0.980941	0.003957	0.722702
-20.465496	-1.744603	0.985946	0.003968	0.722645
-21.796591	-1.647961	0.990950	0.004215	0.722371
-21.537251	-1.692536	0.995955	0.004166	0.722376
-21.894942	-1.633844	1.000960	0.004232	0.722368
-21.823002	-1.643024	1.005965	0.004218	0.722377
-21.928203	-1.628217	1.010970	0.004236	0.722371
-21.783286	-1.653571	1.015974	0.004208	0.722373
-21.343549	-1.730585	1.020979	0.004126	0.722377
-21.840145	-1.647201	1.025984	0.004217	0.722369
-22.121959	-1.726084	1.030989	0.004269	0.722117
-22.462496	-1.688965	1.035994	0.004332	0.722073
-22.830563	-1.621547	1.040998	0.004399	0.722078
-22.701369	-1.644699	1.046003	0.004374	0.722079
-22.713608	-1.648112	1.051008	0.004376	0.722070
-22.350150	-1.708327	1.056013	0.004307	0.722080
-22.692585	-1.651237	1.061018	0.004370	0.722074
-22.665807	-1.673440	1.066022	0.004364	0.722042
-23.344247	-1.701975	1.071027	0.004490	0.721750
-23.591196	-1.663394	1.076032	0.004535	0.721741
-23.696752	-1.640853	1.081037	0.004554	0.721750
-23.309241	-1.713181	1.086042	0.004481	0.721745
-23.691637	-1.646151	1.091046	0.004551	0.721745
-23.699349	-1.643139	1.096051	0.004551	0.721749
-23.251675	-1.728205	1.101056	0.004467	0.721741
-23.353808	-1.792106	1.106061	0.004485	0.721581
-25.036728	-1.567155	1.111066	0.004798	0.721436
-24.573125	-1.648586	1.116070	0.004711	0.721439
-24.319439	-1.691605	1.121075	0.004663	0.721445
-24.719951	-1.627542	1.126080	0.004736	0.721433
-24.575549	-1.649830	1.131085	0.004709	0.721441
-24.671694	-1.637225	1.136090	0.004726	0.721434
-24.620511	-1.644106	1.141094	0.004715	0.721440
-24.681382	-1.728377	1.146099	0.004726	0.721254
-25.637914	-1.627693	1.151104	0.004903	0.721119
-25.009249	-1.737130	1.156109	0.004785	0.721126
-25.262013	-1.695999	1.161114	0.004831	0.721120
-25.718206	-1.615904	1.166118	0.004915	0.721119
-25.314168	-1.686176	1.171123	0.004839	0.721124
-25.663224	-1.630080	1.176128	0.004903	0.721114
-25.525345	-1.670418	1.181133	0.004877	0.721084
-25.750290	-1.737722	1.186138	0.004918	0.720875
-25.826595	-1.725552	1.191142	0.004931	0.720873
-26.276314	-1.640697	1.196147	0.005014	0.720884
-26.235605	-1.653809	1.201152	0.005006	0.720875
-25.687464	-1.747045	1.206157	0.004903	0.720885
-26.488772	-1.607714	1.211162	0.005051	0.720880
-26.315207	-1.722947	1.216166	0.005018	0.720715
-26.731975	-1.735573	1.221171	0.005095	0.720546
-26.833702	-1.724427	1.226176	0.005113	0.720534
-27.321895	-1.632642	1.231181	0.005203	0.720545
-27.273168	-1.644126	1.236186	0.005193	0.720541
-27.068820	-1.681577	1.241190	0.005154	0.720541
-27.029748	-1.687138	1.246195	0.005146	0.720545
-27.251277	-1.725748	1.251200	0.005186	0.720393
-27.948849	-1.685630	1.256205	0.005315	0.720229
-27.914253	-1.697133	1.261210	0.005308	0.720220
-28.387333	-1.614461	1.266214	0.005395	0.720219
-28.028179	-1.674488	1.271219	0.005327	0.720228
-28.043235	-1.677704	1.276224	0.005329	0.720218
-28.038555	-1.674723	1.281229	0.005328	0.720227
-27.970709	-1.706217	1.286234	0.005314	0.720191
-28.640246	-1.736082	1.291238	0.005438	0.719899
-28.921560	-1.685618	1.296243	0.005489	0.719901
-29.325172	-1.617059	1.301248	0.005564	0.719896
-28.553928	-1.751904	1.306253	0.005419	0.719903
-28.733427	-1.723455	1.311258	0.005452	0.719897
-29.359025	-1.612431	1.316262	0.005567	0.719898
-28.758044	-1.717390	1.321267	0.005455	0.719904
-29.613822	-1.707844	1.326272	0.005613	0.719624
-30.119252	-1.627763	1.331277	0.005706	0.719606
-30.006163	-1.650112	1.336282	0.005684	0.719603
-29.654541	-1.716012	1.341286	0.005618	0.719598
-29.835385	-1.680154	1.346291	0.005651	0.719607
-30.237009	-1.614480	1.351296	0.005725	0.719597
-29.520469	-1.738399	1.356301	0.005591	0.719606
-29.915667	-1.744072	1.361306	0.005663	0.719458
-31.332407	-1.587824	1.366310	0.005926	0.719270
-30.514897	-1.731908	1.371315	0.005773	0.719275
-30.831069	-1.681290	1.376320	0.005831	0.719265
-31.045331	-1.638334	1.381325	0.005870	0.719276
-30.744675	-1.695434	1.386330	0.005813	0.719271
-30.860319	-1.675227	1.391334	0.005834	0.719272
-30.748199	-1.695068	1.396339	0.005812	0.719274
-31.515874	-1.715003	1.401344	0.005954	0.718966
-31.623785	-1.696014	1.406349	0.005974	0.718967
-31.701790	-1.685793	1.411354	0.005987	0.718962
-31.676083	-1.689296	1.416358	0.005982	0.718966
-31.474627	-1.725128	1.421363	0.005943	0.718967
-31.878930	-1.658218	1.426368	0.006018	0.718959
-31.793500	-1.670538	1.431373	0.006001	0.718966
-32.147278	-1.716540	1.436378	0.006066	0.718753
-32.905948	-1.637014	1.441382	0.006206	0.718645
-32.406224	-1.725021	1.446387	0.006112	0.718648
-33.170001	-1.594598	1.451392	0.006254	0.718639
-32.971586	-1.625975	1.456397	0.006216	0.718648
-32.512433	-1.710395	1.461402	0.006130	0.718645
-32.833532	-1.655215	1.466406	0.006189	0.718642
-32.884765	-1.642169	1.471411	0.006197	0.718652
-33.048709	-1.751341	1.476416	0.006227	0.718380
-33.696319	-1.646069	1.481421	0.006347	0.718362
-33.942303	-1.606362	1.486426	0.006392	0.718355
-33.514440	-1.684498	1.491430	0.006311	0.718353
-33.373880	-1.708459	1.496435	0.006284	0.718357
-33.796011	-1.638920	1.501440	0.006362	0.718347
-33.243202	-1.733539	1.506445	0.006258	0.718357
-33.673535	-1.778610	1.511450	0.006337	0.718118
-34.989899	-1.599064	1.516454	0.006581	0.718011
-34.481969	-1.685892	1.521459	0.006486	0.718020
-34.401068	-1.706340	1.526464	0.006470	0.718010
-34.759285	-1.637790	1.531469	0.006536	0.718021
-34.707886	-1.650139	1.536474	0.006525	0.718016
-34.674551	-1.658598	1.541478	0.006518	0.718013
-34.250726	-1.770386	1.546483	0.006439	0.717942
-35.726756	-1.633629	1.551488	0.006713	0.717695
-35.273779	-1.710515	1.556493	0.006627	0.717704
-35.386845	-1.692700	1.561498	0.006648	0.717701
-35.664859	-1.645585	1.566502	0.006699	0.717698
-35.571837	-1.658870	1.571507	0.006680	0.717706
-35.882062	-1.608821	1.576512	0.006737	0.717697
-35.512190	-1.672523	1.581517	0.006668	0.717703
-35.664706	-1.738338	1.586522	0.006695	0.717521
-36.738308	-1.621948	1.591526	0.006894	0.717375
-35.974158	-1.755487	1.596531	0.006751	0.717381
-36.469897	-1.673614	1.601536	0.006842	0.717370
-36.509095	-1.663509	1.606541	0.006849	0.717378
-36.278837	-1.705741	1.611546	0.006805	0.717377
-36.786220	-1.617847	1.616550	0.006899	0.717374
-36.704376	-1.652510	1.621555	0.006883	0.717336
-37.186698	-1.698865	1.626560	0.006972	0.717076
-37.086858	-1.712264	1.631565	0.006952	0.717086
-37.548586	-1.631830	1.636570	0.007037	0.717084
-37.464440	-1.648707	1.641574	0.007021	0.717082
-37.077586	-1.715834	1.646579	0.006948	0.717087
-37.678468	-1.611520	1.651584	0.007059	0.717084
-37.508338	-1.640754	1.656589	0.007026	0.717087
-37.437577	-1.764005	1.661594	0.007012	0.716870
-38.576006	-1.621753	1.666598	0.007223	0.716752
-38.115450	-1.699921	1.671603	0.007137	0.716761
-38.396674	-1.656369	1.676608	0.007188	0.716750
-38.480589	-1.636843	1.681613	0.007203	0.716761
-38.108767	-1.705633	1.686618	0.007133	0.716757
-38.453681	-1.647621	1.691622	0.007196	0.716752
-38.332202	-1.717875	1.696627	0.007173	0.716657
-39.576577	-1.605529	1.701632	0.007404	0.716443
-39.106598	-1.686720	1.706637	0.007315	0.716449
-39.195489	-1.672577	1.711642	0.007331	0.716448
-39.654453	-1.593300	1.716646	0.007416	0.716444
-39.192717	-1.670934	1.721651	0.007329	0.716455
-39.232600	-1.671984	1.726656	0.007335	0.716441
-38.975148	-1.715042	1.731661	0.007287	0.716448
-39.420468	-1.763480	1.736666	0.007369	0.716196
-40.548111	-1.598181	1.741670	0.007578	0.716127
-39.911930	-1.708549	1.746675	0.007458	0.716135
-40.053806	-1.690167	1.751680	0.007484	0.716123
-40.425833	-1.620464	1.756685	0.007552	0.716131
-40.130031	-1.675320	1.761690	0.007496	0.716129
-40.003692	-1.700738	1.766694	0.007472	0.716125
-40.108748	-1.741507	1.771699	0.007491	0.716008
-41.229600	-1.608914	1.776704	0.007698	0.715877
-40.754299	-1.690469	1.781709	0.007609	0.715885
-40.696248	-1.703879	1.786714	0.007598	0.715880
-40.969210	-1.656707	1.791718	0.007647	0.715879
-40.660224	-1.709777	1.796723	0.007589	0.715885
-41.035881	-1.646202	1.801728	0.007658	0.715880
-41.501158	-1.685856	1.806733	0.007744	0.715638
-41.952883	-1.653883	1.811738	0.007827	0.715544
-42.075795	-1.634464	1.816742	0.007849	0.715541
-41.894332	-1.663205	1.821747	0.007815	0.715549
-41.969246	-1.655683	1.826752	0.007828	0.715540
-41.734400	-1.696020	1.831757	0.007783	0.715544
-41.914760	-1.663887	1.836762	0.007816	0.715546
-42.194387	-1.654693	1.841766	0.007867	0.715467
-42.549853	-1.708640	1.846771	0.007932	0.715236
-42.441199	-1.733541	1.851776	0.007911	0.715227
-43.299459	-1.579304	1.856781	0.008070	0.715231
-42.987127	-1.635887	1.861786	0.008011	0.715231
-42.752415	-1.681003	1.866790	0.007967	0.715226
-42.754628	-1.677261	1.871795	0.007966	0.715234
-43.057562	-1.627738	1.876800	0.008022	0.715227
-43.421749	-1.710728	1.881805	0.008089	0.714935
-43.613463	-1.691478	1.886810	0.008123	0.714907
-43.938979	-1.635766	1.891814	0.008183	0.714904
-43.394786	-1.727560	1.896819	0.008081	0.714916
-43.780353	-1.665712	1.901824	0.008152	0.714904
-44.001322	-1.623787	1.906829	0.008192	0.714911
-43.377112	-1.737309	1.911834	0.008075	0.714908
-44.209801	-1.712588	1.916838	0.008229	0.714664
-44.648967	-1.659114	1.921843	0.008310	0.714617
-44.783783	-1.641344	1.926848	0.008334	0.714606
-44.361053	-1.715278	1.931853	0.008255	0.714610
-44.596667	-1.675934	1.936858	0.008298	0.714607
-45.054826	-1.595685	1.941862	0.008382	0.714605
-44.454790	-1.701050	1.946867	0.008270	0.714610
-44.514960	-1.779711	1.951872	0.008280	0.714434
-45.929571	-1.607575	1.956877	0.008543	0.714277
-45.639379	-1.661670	1.961882	0.008488	0.714274
-45.701444	-1.653676	1.966886	0.008498	0.714270
-45.740905	-1.643305	1.971891	0.008505	0.714278
-45.663598	-1.662577	1.976896	0.008490	0.714269
-45.456525	-1.695342	1.981901	0.008450	0.714279
-45.378132	-1.730249	1.986906	0.008435	0.714239
-46.632694	-1.646184	1.991910	0.008668	0.713963
-46.342251	-1.694119	1.996915	0.008613	0.713972
-46.629089	-1.647204	2.001920	0.008665	0.713966
-46.338846	-1.698790	2.011917	0.008609	0.713969
-46.611404	-1.651837	2.021914	0.008658	0.713969
-46.383837	-1.694262	2.031910	0.008614	0.713969
-46.626960	-1.652592	2.041907	0.008658	0.713969
-46.731888	-1.694445	2.051904	0.008676	0.713852
-46.978385	-1.594569	2.061901	0.008720	0.713966
-46.442564	-1.691246	2.071898	0.008618	0.713967
-46.516696	-1.678346	2.081894	0.008630	0.713970
-46.816323	-1.627553	2.091891	0.008685	0.713968
-46.504285	-1.685696	2.101888	0.008625	0.713966
-46.535664	-1.683285	2.111885	0.008629	0.713963
-46.546981	-1.681774	2.121882	0.008629	0.713965
-46.537545	-1.683763	2.131878	0.008626	0.713968
-46.129419	-1.654171	2.141875	0.008548	0.714174
-45.718890	-1.679940	2.151872	0.008470	0.714272
-45.641639	-1.697000	2.161869	0.008454	0.714269
-45.508795	-1.719717	2.171866	0.008427	0.714274
-45.570730	-1.710485	2.181862	0.008437	0.714273
-45.113534	-1.644523	2.191859	0.008350	0.714569
-44.722376	-1.699836	2.201856	0.008276	0.714601
-44.594422	-1.724631	2.211853	0.008250	0.714601
-44.939059	-1.662437	2.221850	0.008313	0.714605
-44.153472	-1.679240	2.231846	0.008165	0.714853
-44.010864	-1.680185	2.241843	0.008136	0.714905
-43.853589	-1.710912	2.251840	0.008105	0.714903
-44.103264	-1.662328	2.261837	0.008150	0.714914
-43.362718	-1.636931	2.271834	0.008011	0.715230
-43.140103	-1.677880	2.281830	0.007967	0.715230
-43.171817	-1.673521	2.291827	0.007972	0.715231
-42.857735	-1.647310	2.301824	0.007911	0.715397
-42.486024	-1.643249	2.311821	0.007840	0.715540
-42.090328	-1.713848	2.321818	0.007765	0.715543
-42.246289	-1.686803	2.331814	0.007792	0.715545
-41.681277	-1.623437	2.341811	0.007685	0.715873
-41.519860	-1.650051	2.351808	0.007654	0.715881
-41.506769	-1.655014	2.361805	0.007649	0.715879
-40.903888	-1.695235	2.371802	0.007536	0.716015
-40.574061	-1.696465	2.381798	0.007472	0.716132
-40.648572	-1.686849	2.391795	0.007485	0.716128
-40.591010	-1.690700	2.401792	0.007472	0.716144
-40.036875	-1.639771	2.411789	0.007367	0.716444
-39.459166	-1.742391	2.421786	0.007258	0.716448
-39.732965	-1.695382	2.431782	0.007307	0.716447
-39.557147	-1.637914	2.441779	0.007273	0.716627
-39.015191	-1.672255	2.451776	0.007170	0.716753
-39.095888	-1.658460	2.461773	0.007183	0.716755
-38.781814	-1.656896	2.471770	0.007123	0.716872
-38.102889	-1.672830	2.481766	0.006995	0.717083
-38.093049	-1.677334	2.491763	0.006992	0.717081
-38.222371	-1.650926	2.501760	0.007014	0.717091
-37.515100	-1.634646	2.511757	0.006880	0.717375
-37.174053	-1.695853	2.521754	0.006815	0.717378
-37.380261	-1.661085	2.531750	0.006852	0.717377
-36.867065	-1.635042	2.541747	0.006755	0.717613
-36.710848	-1.621179	2.551744	0.006724	0.717698
-36.353759	-1.686071	2.561741	0.006656	0.717699
-36.275871	-1.629540	2.571738	0.006639	0.717841
-35.518433	-1.676665	2.581734	0.006497	0.718018
-35.581421	-1.669544	2.591731	0.006507	0.718013
-35.668588	-1.648740	2.601728	0.006521	0.718027
-34.838079	-1.634100	2.611725	0.006365	0.718351
-34.491564	-1.696987	2.621722	0.006299	0.718352
-34.944024	-1.619312	2.631718	0.006381	0.718350
-34.141983	-1.669876	2.641715	0.006230	0.718535
-34.184252	-1.610980	2.651712	0.006236	0.718640
-34.046493	-1.636923	2.661709	0.006209	0.718640
-33.918943	-1.602760	2.671706	0.006183	0.718756
-33.027625	-1.659499	2.681702	0.006016	0.718960
-33.080525	-1.651564	2.691699	0.006024	0.718961
-33.442508	-1.577608	2.701696	0.006089	0.718982
-32.315295	-1.635031	2.711693	0.005878	0.719268
-32.177543	-1.660772	2.721690	0.005850	0.719269
-32.263933	-1.646239	2.731686	0.005865	0.719271
-31.745484	-1.624040	2.741683	0.005767	0.719500
-31.574170	-1.606557	2.751680	0.005733	0.719598
-31.119203	-1.687920	2.761677	0.005647	0.719600
-31.395573	-1.607593	2.771674	0.005696	0.719665
-30.516127	-1.647235	2.781670	0.005531	0.719899
-30.680653	-1.621563	2.791667	0.005560	0.719895
-30.712665	-1.617030	2.801664	0.005564	0.719896
-29.746401	-1.637647	2.811661	0.005382	0.720197
-29.737501	-1.629923	2.821658	0.005379	0.720219
-29.565164	-1.662298	2.831654	0.005345	0.720219
-29.433352	-1.610656	2.841651	0.005319	0.720370
-28.923753	-1.618890	2.851648	0.005222	0.720536
-28.714022	-1.658201	2.861645	0.005181	0.720535
-28.724965	-1.657936	2.871642	0.005182	0.720535
-27.795318	-1.657303	2.881638	0.005007	0.720865
-27.879968	-1.638907	2.891635	0.005021	0.720875
-27.841232	-1.648284	2.901632	0.005012	0.720873
-27.953264	-1.585327	2.911629	0.005031	0.720961
-27.249052	-1.631954	2.921626	0.004898	0.721119
-27.017861	-1.675364	2.931622	0.004854	0.721118
-27.239092	-1.616552	2.941619	0.004893	0.721160
-26.466491	-1.616379	2.951616	0.004748	0.721434
-26.103840	-1.684032	2.961613	0.004678	0.721431
-26.309119	-1.647890	2.971610	0.004715	0.721433
-25.555583	-1.662160	2.981606	0.004573	0.721672
-25.602587	-1.619561	2.991603	0.004580	0.721743
-25.424329	-1.654140	3.001600	0.004545	0.721740
-25.246356	-1.624349	3.011597	0.004510	0.721864
-24.482836	-1.655200	3.021594	0.004366	0.722074
-24.367830	-1.678835	3.031590	0.004343	0.722071
-24.722797	-1.614687	3.041587	0.004407	0.722076
-23.912138	-1.618787	3.051584	0.004255	0.722355
-23.701725	-1.652284	3.061581	0.004214	0.722366
-23.837467	-1.627848	3.071578	0.004237	0.722369
-23.226507	-1.632925	3.081574	0.004122	0.722576
-22.876877	-1.638996	3.091571	0.004055	0.722690
-22.910384	-1.635073	3.101568	0.004060	0.722689
-22.977644	-1.584194	3.111565	0.004070	0.722768
-21.950293	-1.646052	3.121562	0.003877	0.723009
-21.806570	-1.672967	3.131558	0.003849	0.723010
-21.929261	-1.653643	3.141555	0.003870	0.723008
-21.244047	-1.648400	3.151552	0.003741	0.723261
-20.951223	-1.657971	3.161549	0.003684	0.723347
-20.988542	-1.650180	3.171546	0.003690	0.723353
-20.871585	-1.668343	3.181542	0.003666	0.723361
-20.372389	-1.612123	3.191539	0.003572	0.723649
-20.113460	-1.658112	3.201536	0.003522	0.723652
-20.249687	-1.638015	3.211533	0.003545	0.723647
-19.834153	-1.616311	3.221530	0.003466	0.723838
-19.059115	-1.677340	3.231526	0.003320	0.723992
-19.235921	-1.648344	3.241523	0.003351	0.723990
-18.984401	-1.693930	3.251520	0.003303	0.723992
-18.608187	-1.610966	3.261517	0.003231	0.724289
-18.247188	-1.659793	3.271514	0.003162	0.724322
-18.140775	-1.677308	3.281510	0.003141	0.724328
-18.222263	-1.613580	3.291507	0.003154	0.724428
-17.062404	-1.700108	3.301504	0.002936	0.724666
-17.262585	-1.665155	3.311501	0.002972	0.724668
-17.264914	-1.666864	3.321498	0.002971	0.724667
-16.890546	-1.658457	3.331494	0.002899	0.724817
-16.336724	-1.678424	3.341491	0.002794	0.724974
-16.262179	-1.695816	3.351488	0.002779	0.724969
-16.542533	-1.646072	3.361485	0.002829	0.724972
-15.709375	-1.674376	3.371482	0.002672	0.725210
-15.648996	-1.645753	3.381478	0.002659	0.725290
-15.450068	-1.685169	3.391475	0.002621	0.725285
-15.473242	-1.645625	3.401472	0.002623	0.725358
-14.534916	-1.694059	3.411469	0.002447	0.725593
-14.712561	-1.664319	3.421466	0.002478	0.725592
-14.793988	-1.649748	3.431462	0.002492	0.725596
-14.197227	-1.635173	3.441459	0.002379	0.725835
-13.922178	-1.638844	3.451456	0.002326	0.725927
-14.113870	-1.606645	3.461453	0.002360	0.725926
-13.482779	-1.666925	3.471450	0.002241	0.726031
-12.877074	-1.689932	3.481446	0.002126	0.726200
-12.759011	-1.713633	3.491443	0.002102	0.726198
-13.113600	-1.653358	3.501440	0.002167	0.726195
-12.228822	-1.681932	3.511437	0.002000	0.726450
-12.017858	-1.689411	3.521434	0.001959	0.726512
-12.143187	-1.669386	3.531430	0.001981	0.726511
-12.045052	-1.640796	3.541427	0.001961	0.726604
-11.302664	-1.664138	3.551424	0.001821	0.726819
-11.308993	-1.665296	3.561421	0.001820	0.726818
-11.190831	-1.687132	3.571418	0.001797	0.726820
-10.631507	-1.635003	3.581414	0.001691	0.727119
-10.098330	-1.720567	3.591411	0.001590	0.727140
-10.124941	-1.717153	3.601408	0.001593	0.727141
-10.126986	-1.683476	3.611405	0.001592	0.727209
-9.340760	-1.708702	3.621402	0.001444	0.727436
-9.363397	-1.705555	3.631398	0.001446	0.727437
-9.301059	-1.719177	3.641395	0.001433	0.727436
-9.010104	-1.661825	3.651392	0.001377	0.727651
-8.606952	-1.686843	3.661389	0.001300	0.727746
-8.361941	-1.728605	3.671386	0.001253	0.727752
-8.441232	-1.691460	3.681382	0.001266	0.727801
-7.504370	-1.725731	3.691379	0.001090	0.728062
-7.611938	-1.709554	3.701376	0.001108	0.728059
-7.534387	-1.724398	3.711373	0.001092	0.728060
-7.184641	-1.705513	3.721370	0.001025	0.728221
-6.515160	-1.734399	3.731366	0.000899	0.728400
-6.520827	-1.738327	3.741363	0.000898	0.728394
-6.750866	-1.698507	3.751360	0.000939	0.728395
-6.015627	-1.701029	3.761357	0.000800	0.728648
-5.903466	-1.696159	3.771354	0.000778	0.728699
-5.802450	-1.715139	3.781350	0.000757	0.728701
-5.405611	-1.741244	3.791347	0.000682	0.728790
-4.843317	-1.724002	3.801344	0.000575	0.729022
-4.859380	-1.723149	3.811341	0.000576	0.729021
-4.907005	-1.715874	3.821338	0.000584	0.729022
-4.310913	-1.719846	3.831334	0.000471	0.729224
-4.225511	-1.680595	3.841331	0.000453	0.729333
-4.200477	-1.687940	3.851328	0.000447	0.729330
-3.887345	-1.703487	3.861325	0.000387	0.729411
-3.368296	-1.672485	3.871322	0.000288	0.729654
-3.130029	-1.717054	3.881318	0.000242	0.729653
-3.033109	-1.736590	3.891315	0.000223	0.729652
-2.699986	-1.672133	3.901312	0.000159	0.729896
-2.687934	-1.647909	3.911309	0.000155	0.729950
-2.354610	-1.708871	3.921306	0.000091	0.729950
-2.659041	-1.560815	3.931302	0.000146	0.730135
-1.902694	-1.628729	3.941299	0.000003	0.730268
-2.148348	-1.585409	3.951296	0.000047	0.730270
-2.143053	-1.454446	3.961293	0.000045	0.730530
-0.913919	-1.649398	3.971290	-0.000186	0.730579
-1.588863	-1.520782	3.981286	-0.000062	0.730599
-1.251218	-1.417624	3.991283	-0.000127	0.730918
-1.141620	-1.440704	4.001280	-0.000149	0.730915
-1.522862	-1.278009	4.011277	-0.000079	0.731102
-1.119408	-1.298831	4.021274	-0.000156	0.731204
-1.474177	-1.140285	4.031270	-0.000092	0.731392
-0.994951	-1.161984	4.041267	-0.000183	0.731518
-0.581374	-1.121433	4.051264	-0.000262	0.731743
-0.712999	-1.057568	4.061261	-0.000239	0.731824
-0.910456	-0.880470	4.071258	-0.000204	0.732102
-0.830709	-0.831626	4.081254	-0.000221	0.732227
-0.316107	-0.809338	4.091251	-0.000318	0.732451
-1.023772	-0.580528	4.101248	-0.000188	0.732653
-0.617281	-0.559019	4.111245	-0.000266	0.732838
-0.584149	-0.441144	4.121242	-0.000274	0.733080
-0.198726	-0.363260	4.131238	-0.000347	0.733366
-0.106092	-0.285530	4.141235	-0.000366	0.733552
-0.018433	-0.200578	4.151232	-0.000384	0.733749
0.059540	-0.073927	4.161229	-0.000401	0.734024
0.261933	0.021047	4.171226	-0.000440	0.734280
0.000000	0.214557	4.181222	-0.000393	0.734566
-0.299185	0.912829	4.186227	-0.000339	0.735811
0.038555	2.123458	4.191232	-0.000403	0.738256
1.150258	3.817902	4.196237	-0.000612	0.741881
2.147153	6.097475	4.201242	-0.000800	0.746561
3.459944	8.868570	4.206246	-0.001047	0.752244
4.615171	12.145707	4.211251	-0.001266	0.758777
6.246278	15.797954	4.216256	-0.001573	0.766105
8.671226	19.781041	4.221261	-0.002027	0.774226
11.222991	24.132384	4.226266	-0.002506	0.782970
13.905058	28.879155	4.231270	-0.003010	0.792364
15.923152	34.097455	4.236275	-0.003390	0.802273
18.733267	39.517808	4.241280	-0.003917	0.812656
21.595196	45.272300	4.246285	-0.004455	0.823498
23.472567	51.514563	4.251290	-0.004809	0.834730
25.332324	57.991397	4.256294	-0.005161	0.846199
26.508346	64.835436	4.261299	-0.005385	0.857922
27.306560	71.952085	4.266304	-0.005539	0.869821
28.206075	79.244151	4.271309	-0.005712	0.881870
29.069723	86.712611	4.276314	-0.005879	0.894025
30.075807	94.322812	4.281318	-0.006072	0.906277
31.411043	102.029343	4.286323	-0.006326	0.918603
32.336230	109.928366	4.291328	-0.006505	0.930948
34.064668	117.817085	4.296333	-0.006833	0.943327
36.528822	125.705295	4.301338	-0.007297	0.955734
37.450415	133.950279	4.306342	-0.007475	0.968108
38.267468	142.298459	4.311347	-0.007634	0.980449
39.198423	150.716601	4.316352	-0.007813	0.992763
40.209769	159.145390	4.321357	-0.008008	1.004961
41.411355	167.583638	4.326362	-0.008238	1.017071
42.415756	176.108683	4.331366	-0.008432	1.029111
43.620984	184.628912	4.336371	-0.008662	1.041051
44.432405	193.246481	4.341376	-0.008820	1.052894
45.674057	201.824146	4.346381	-0.009058	1.064651
46.543045	210.491632	4.351386	-0.009226	1.076313
47.852950	219.073076	4.356390	-0.009476	1.087836
48.564019	227.774609	4.361395	-0.009615	1.099259
49.093378	236.498242	4.366400	-0.009720	1.110552
50.089688	245.141885	4.371405	-0.009912	1.121732
50.833851	253.815710	4.376410	-0.010057	1.132785
51.507856	262.508031	4.381414	-0.010189	1.143738
52.058069	271.246373	4.386419	-0.010298	1.154618
52.601060	279.902031	4.391424	-0.010406	1.165294
53.501103	288.517974	4.396429	-0.010580	1.175898
53.950562	297.167064	4.401434	-0.010670	1.186355
54.633680	305.791325	4.406438	-0.010804	1.196738
55.397360	314.366126	4.411443	-0.010953	1.206989
56.158511	322.941368	4.416448	-0.011101	1.217154
56.722050	331.541851	4.421453	-0.011212	1.227224
56.967578	340.180794	4.426458	-0.011264	1.237195
57.781470	348.683926	4.431462	-0.011422	1.247041
58.561327	357.202745	4.436467	-0.011574	1.256820
59.008148	365.742886	4.441472	-0.011664	1.266485
59.753109	374.248563	4.446477	-0.011809	1.276093
60.333318	382.734950	4.451482	-0.011923	1.285578
61.045258	391.219505	4.456486	-0.012062	1.295015
61.685322	399.679952	4.461491	-0.012188	1.304345
62.390137	408.226032	4.466496	-0.012325	1.313711
62.779965	416.711707	4.471501	-0.012404	1.322890
63.380326	425.113928	4.476506	-0.012522	1.331955
64.195081	433.484266	4.481510	-0.012680	1.340962
64.462327	441.940040	4.486515	-0.012737	1.349902
64.862648	450.348609	4.491520	-0.012817	1.358757
65.410948	458.733661	4.496525	-0.012926	1.367556
65.906494	467.114114	4.501530	-0.013024	1.376285
66.394272	475.485288	4.506534	-0.013122	1.384947
67.112111	483.839399	4.511539	-0.013262	1.393577
67.711260	492.161396	4.516544	-0.013379	1.402102
68.216794	500.519536	4.521549	-0.013480	1.410595
68.641217	508.861033	4.526554	-0.013565	1.419007
69.250077	517.175817	4.531558	-0.013685	1.427373
69.515368	525.550271	4.536563	-0.013741	1.435693
69.864821	533.868140	4.541568	-0.013812	1.443924
70.522396	542.166685	4.546573	-0.013941	1.452138
70.725795	550.506786	4.551578	-0.013985	1.460273
70.986261	558.848594	4.556582	-0.014040	1.468374
71.545730	567.160200	4.561587	-0.014150	1.476448
71.872719	575.429247	4.566592	-0.014217	1.484402
72.666802	583.669080	4.571597	-0.014371	1.492358
72.818944	591.964301	4.576602	-0.014406	1.500224
73.322841	600.226825	4.581606	-0.014506	1.508073
73.675713	608.514893	4.586611	-0.014578	1.515881
73.960292	616.771415	4.591616	-0.014637	1.523610
74.569756	624.996370	4.596621	-0.014757	1.531319
75.002479	633.245413	4.601626	-0.014844	1.538986
75.251644	641.515086	4.606630	-0.014896	1.546605
75.696720	649.777562	4.611635	-0.014985	1.554210
76.288226	657.962637	4.616640	-0.015102	1.561729
76.791081	666.185969	4.621645	-0.015202	1.569233
76.999968	674.447678	4.626650	-0.015247	1.576693
77.373839	682.675744	4.631654	-0.015323	1.584111
77.662347	690.922894	4.636659	-0.015382	1.591500
77.875155	699.157234	4.641664	-0.015428	1.598832
78.455931	707.335342	4.646669	-0.015543	1.606133
78.817308	715.566257	4.651674	-0.015616	1.613416
79.009518	723.794846	4.656678	-0.015658	1.620641
79.699641	731.959606	4.661683	-0.015793	1.627848
80.359048	740.179995	4.666688	-0.015922	1.635066
80.908774	748.355848	4.671693	-0.016030	1.642199
81.101283	756.570024	4.676698	-0.016072	1.649284
81.481262	764.763088	4.681702	-0.016149	1.656347
81.962492	772.935473	4.686707	-0.016245	1.663376
82.311972	781.126112	4.691712	-0.016316	1.670373
82.701669	789.334778	4.696717	-0.016395	1.677361
83.022688	797.505726	4.701722	-0.016461	1.684279
83.173084	805.730731	4.706726	-0.016495	1.691192
83.462174	813.926082	4.711731	-0.016555	1.698070
84.018764	822.064453	4.716736	-0.016665	1.704907
84.351257	830.276902	4.721741	-0.016733	1.711749
84.312514	838.501900	4.726746	-0.016732	1.718527
84.758635	846.626625	4.731750	-0.016822	1.725257
85.239837	854.788203	4.736755	-0.016917	1.731996
85.363270	862.980980	4.741760	-0.016947	1.738689
85.774645	871.126316	4.746765	-0.017029	1.745354
86.459403	879.240775	4.751770	-0.017163	1.752003
86.940012	887.388371	4.756774	-0.017259	1.758627
87.462378	895.503404	4.761779	-0.017362	1.765206
87.647241	903.690091	4.766784	-0.017403	1.771775
88.005621	911.864297	4.771789	-0.017476	1.778332
88.437926	919.984079	4.776794	-0.017562	1.784830
88.673774	928.211260	4.781798	-0.017612	1.791365
89.114392	936.373511	4.786803	-0.017701	1.797851
89.275386	944.504987	4.791808	-0.017737	1.804254
90.027627	952.597953	4.796813	-0.017883	1.810677
90.151071	960.776535	4.801818	-0.017912	1.817067
90.579169	968.896836	4.806822	-0.017998	1.823427
90.800084	977.079033	4.811827	-0.018045	1.829787
91.171533	985.201925	4.816832	-0.018121	1.836097
91.671437	993.319584	4.821837	-0.018220	1.842397
91.781834	1001.475662	4.826842	-0.018247	1.848659
92.252865	1009.609207	4.831846	-0.018340	1.854925
92.696081	1017.721751	4.836851	-0.018429	1.861150
93.092894	1025.835787	4.841856	-0.018509	1.867350
93.488576	1034.011074	4.846861	-0.018589	1.873575
93.748391	1042.138342	4.851866	-0.018644	1.879728
94.180014	1050.235959	4.856870	-0.018730	1.885858
94.413060	1058.395534	4.861875	-0.018780	1.891992
94.555449	1066.550528	4.866880	-0.018812	1.898093
94.869912	1074.670929	4.871885	-0.018877	1.904167
95.122247	1082.802085	4.876890	-0.018930	1.910223
95.600745	1090.909233	4.881894	-0.019025	1.916268
96.366925	1098.956747	4.886899	-0.019174	1.922281
96.414407	1107.116601	4.891904	-0.019189	1.928278
96.724540	1115.272841	4.896909	-0.019253	1.934283
96.996944	1123.384981	4.901914	-0.019310	1.940233
97.571981	1131.462643	4.906918	-0.019423	1.946172
98.559289	1139.562296	4.911923	-0.019613	1.952154
98.857029	1147.692585	4.916928	-0.019675	1.958066
99.327343	1155.780262	4.921933	-0.019769	1.963947
99.490455	1163.912620	4.926938	-0.019805	1.969809
100.099817	1171.999946	4.931942	-0.019925	1.975670
100.765314	1180.071071	4.936947	-0.020055	1.981507
101.141854	1188.176441	4.941952	-0.020131	1.987321
101.417604	1196.343098	4.946957	-0.020188	1.993150
101.773583	1204.443420	4.951962	-0.020261	1.998924
102.078820	1212.546222	4.956966	-0.020324	2.004678
102.278015	1220.691385	4.961971	-0.020367	2.010434
102.506923	1228.813158	4.966976	-0.020416	2.016160
102.727674	1236.929959	4.971981	-0.020463	2.021865
102.779671	1245.057152	4.976986	-0.020479	2.027545
103.362448	1253.153971	4.981990	-0.020594	2.033241
104.685490	1261.122130	4.986995	-0.020846	2.038908
104.947807	1269.219629	4.992000	-0.020901	2.044540
105.171186	1277.356497	4.997005	-0.020949	2.050180
105.380592	1285.495994	5.002010	-0.020994	2.055805
105.741212	1293.591460	5.007014	-0.021067	2.061400
105.933588	1301.708915	5.012019	-0.021109	2.066977
106.280788	1309.817416	5.017024	-0.021180	2.072549
106.875404	1317.881236	5.022029	-0.021297	2.078100
107.079759	1325.967028	5.027034	-0.021341	2.083612
107.129898	1334.116200	5.032038	-0.021357	2.089137
107.365070	1342.244431	5.037043	-0.021406	2.094652
107.613774	1350.323893	5.042048	-0.021459	2.100121
108.093773	1358.380232	5.047053	-0.021554	2.105582
108.381270	1366.521603	5.052058	-0.021614	2.111067
108.610399	1374.658680	5.057062	-0.021663	2.116530
109.050435	1382.714158	5.062067	-0.021751	2.121944
109.246512	1390.777026	5.067072	-0.021794	2.127326
109.646784	1398.876137	5.072077	-0.021874	2.132738
110.010206	1406.945692	5.077082	-0.021948	2.138113
110.248113	1415.033707	5.082086	-0.021998	2.143475
110.487769	1423.141922	5.087091	-0.022049	2.148836
110.704240	1431.239159	5.092096	-0.022096	2.154175
111.069931	1439.292906	5.097101	-0.022170	2.159487
111.317257	1447.365706	5.102106	-0.022222	2.164786
111.866488	1455.417439	5.107110	-0.022330	2.170087
112.331807	1463.509863	5.112115	-0.022423	2.175393
112.701608	1471.564418	5.117120	-0.022498	2.180653
113.118431	1479.650400	5.122125	-0.022582	2.185925
113.363987	1487.760861	5.127130	-0.022634	2.191184
113.521825	1495.888360	5.132134	-0.022669	2.196433
113.985638	1503.931928	5.137139	-0.022762	2.201644
114.225413	1511.998935	5.142144	-0.022813	2.206837
114.406616	1520.120018	5.147149	-0.022852	2.212047
114.545225	1528.217147	5.152154	-0.022884	2.217226
115.009707	1536.260577	5.157158	-0.022977	2.222388
115.535572	1544.326514	5.162163	-0.023081	2.227557
115.853176	1552.406444	5.167168	-0.023146	2.232705
116.516658	1560.457912	5.172173	-0.023276	2.237853
116.780517	1568.519014	5.177178	-0.023331	2.242960
117.069333	1576.620301	5.182182	-0.023391	2.248083
117.641900	1584.685114	5.187187	-0.023504	2.253196
117.815969	1592.774899	5.192192	-0.023542	2.258278
118.164966	1600.849017	5.197197	-0.023613	2.263354
118.295902	1608.960216	5.202202	-0.023644	2.268424
118.426049	1617.124946	5.207206	-0.023674	2.273514
118.803786	1625.180211	5.212211	-0.023751	2.278547
119.037372	1633.207856	5.217216	-0.023800	2.283539
119.511410	1641.249190	5.222221	-0.023895	2.288550
119.857657	1649.326837	5.227226	-0.023965	2.293560
119.937158	1657.417915	5.232230	-0.023986	2.298546
120.240594	1665.470193	5.237235	-0.024049	2.303515
120.844379	1673.489237	5.242240	-0.024167	2.308479
121.516283	1681.556019	5.247245	-0.024299	2.313467
121.882012	1689.625135	5.252250	-0.024373	2.318419
122.191254	1697.695345	5.257254	-0.024437	2.323357
122.619577	1705.766471	5.262259	-0.024522	2.328295
122.690132	1713.876122	5.267264	-0.024542	2.333217
122.965293	1721.960177	5.272269	-0.024599	2.338129
123.234279	1730.027318	5.277274	-0.024655	2.343020
123.532725	1738.079500	5.282278	-0.024717	2.347894
123.736133	1746.203606	5.287283	-0.024761	2.352794
124.057119	1754.245545	5.292288	-0.024827	2.357643
124.321469	1762.308516	5.297293	-0.024882	2.362491
124.619597	1770.361453	5.302298	-0.024944	2.367325
125.276909	1778.379618	5.307302	-0.025072	2.372157
125.362335	1786.491903	5.312307	-0.025094	2.376990
125.512632	1794.576798	5.317312	-0.025129	2.381802
125.806423	1802.626503	5.322317	-0.025189	2.386594
126.000567	1810.699048	5.327322	-0.025232	2.391383
126.224207	1818.780271	5.332326	-0.025279	2.396169
126.528170	1826.827836	5.337331	-0.025342	2.400933
126.704303	1834.870590	5.342336	-0.025381	2.405673
127.114721	1842.937361	5.347341	-0.025464	2.410437
127.253457	1851.035876	5.352346	-0.025495	2.415189
127.582968	1859.078360	5.357350	-0.025563	2.419914
127.752490	1867.157155	5.362355	-0.025601	2.424638
127.800908	1875.232926	5.367360	-0.025616	2.429342
128.197740	1883.375277	5.372365	-0.025696	2.434101
128.402417	1891.399041	5.377370	-0.025740	2.438769
128.726149	1899.401055	5.382374	-0.025806	2.443423
129.248699	1907.433293	5.387379	-0.025910	2.448102
129.410497	1915.499549	5.392384	-0.025946	2.452763
129.767427	1923.564135	5.397389	-0.026019	2.457430
130.054283	1931.604199	5.402394	-0.026078	2.462068
130.213457	1939.667839	5.407398	-0.026114	2.466701
130.631781	1947.732638	5.412403	-0.026198	2.471346
130.894577	1955.786883	5.417408	-0.026253	2.475964
131.424128	1963.813725	5.422413	-0.026358	2.480578
131.796892	1971.863844	5.427418	-0.026433	2.485185
131.823920	1979.954409	5.432422	-0.026444	2.489780
131.899335	1988.063893	5.437427	-0.026464	2.494382
132.219192	1996.095236	5.442432	-0.026530	2.498948
132.481600	2004.155534	5.447437	-0.026585	2.503518
132.818002	2012.212615	5.452442	-0.026654	2.508084
133.026078	2020.305547	5.457446	-0.026699	2.512652
133.384117	2028.367659	5.462451	-0.026772	2.517205
133.169951	2036.431552	5.467456	-0.026738	2.521710
133.468658	2044.461404	5.472461	-0.026799	2.526224
133.715419	2052.515813	5.477466	-0.026852	2.530740
133.826583	2060.591431	5.482470	-0.026878	2.535251
134.224401	2068.624208	5.487475	-0.026959	2.539750
134.621933	2076.630179	5.492480	-0.027039	2.544225
134.929783	2084.694017	5.497485	-0.027102	2.548719
135.133898	2092.773309	5.502490	-0.027146	2.553206
135.371547	2100.818880	5.507494	-0.027197	2.557669
136.178515	2108.803838	5.512499	-0.027353	2.562130
136.263716	2116.868241	5.517504	-0.027375	2.566577
136.597297	2124.934427	5.522509	-0.027443	2.571034
136.841463	2133.038040	5.527514	-0.027495	2.575498
137.026777	2141.073425	5.532518	-0.027535	2.579913
137.149405	2149.151991	5.537523	-0.027564	2.584339
137.338277	2157.207575	5.542528	-0.027606	2.588750
137.815646	2165.401487	5.547533	-0.027701	2.593248
137.989744	2173.445335	5.552538	-0.027739	2.597636
138.146116	2181.434058	5.557542	-0.027774	2.601986
138.421956	2189.451347	5.562547	-0.027832	2.606351
138.657072	2197.472309	5.567552	-0.027882	2.610709
139.077959	2205.538414	5.572557	-0.027966	2.615096
139.280133	2213.551017	5.577562	-0.028010	2.619433
139.406768	2221.588694	5.582566	-0.028040	2.623770
139.844741	2229.642275	5.587571	-0.028127	2.628130
140.704445	2237.624023	5.592576	-0.028293	2.632471
141.427453	2245.655836	5.597581	-0.028434	2.636823
141.564347	2253.715296	5.602586	-0.028466	2.641144
141.727933	2261.768683	5.607590	-0.028502	2.645457
142.109454	2269.828245	5.612595	-0.028579	2.649780
142.234891	2277.916395	5.617600	-0.028609	2.654094
142.456634	2285.977809	5.622605	-0.028656	2.658393
142.752886	2294.016832	5.627610	-0.028718	2.662679
142.949817	2302.060442	5.632614	-0.028760	2.666953
143.180684	2310.153717	5.637619	-0.028809	2.671249
143.122924	2318.250820	5.642624	-0.028805	2.675521
143.431732	2326.246499	5.647629	-0.028868	2.679757
143.602245	2334.281838	5.652634	-0.028906	2.683998
143.695280	2342.345894	5.657638	-0.028930	2.688242
144.006078	2350.390547	5.662643	-0.028994	2.692483
144.387175	2358.410391	5.667648	-0.029071	2.696709
144.561068	2366.467951	5.672653	-0.029109	2.700935
144.891369	2374.479390	5.677658	-0.029177	2.705140
144.996940	2382.543601	5.682662	-0.029203	2.709352
145.232199	2390.643331	5.687667	-0.029252	2.713584
145.565774	2398.658761	5.692672	-0.029321	2.717772
145.912511	2406.686390	5.697677	-0.029391	2.721960
146.089203	2414.741406	5.702682	-0.029430	2.726145
146.134562	2422.781644	5.707686	-0.029445	2.730308
146.440225	2430.845041	5.712691	-0.029508	2.734493
146.434375	2438.901539	5.717696	-0.029513	2.738649
146.634659	2446.930137	5.722701	-0.029556	2.742796
146.765056	2454.989589	5.727706	-0.029587	2.746949
147.049975	2463.051632	5.732710	-0.029646	2.751107
147.489388	2471.180386	5.737715	-0.029734	2.755301
147.693172	2479.155992	5.742720	-0.029778	2.759396
148.050221	2487.145159	5.747725	-0.029850	2.763502
148.344058	2495.163001	5.752730	-0.029911	2.767612
148.212375	2503.250025	5.757734	-0.029893	2.771726
148.594700	2511.293326	5.762739	-0.029970	2.775842
148.857957	2519.305477	5.767744	-0.030025	2.779929
149.008386	2527.348855	5.772749	-0.030059	2.784019
149.227717	2535.399859	5.777754	-0.030106	2.788111
149.605993	2543.424640	5.782758	-0.030183	2.792193
149.838836	2551.507283	5.787763	-0.030232	2.796290
149.855910	2559.548797	5.792768	-0.030242	2.800347
150.376872	2567.533345	5.797773	-0.030345	2.804399
150.628296	2575.584375	5.802778	-0.030398	2.808463
150.711367	2583.662210	5.807782	-0.030419	2.812525
151.020142	2591.712178	5.812787	-0.030483	2.816580
151.231279	2599.742686	5.817792	-0.030528	2.820613
151.399408	2607.777861	5.822797	-0.030566	2.824641
151.469358	2615.854586	5.827802	-0.030585	2.828678
151.817560	2623.904928	5.832806	-0.030656	2.832712
152.303128	2631.934382	5.837811	-0.030752	2.836737
152.330427	2639.977285	5.842816	-0.030763	2.840738
152.665018	2647.972176	5.847821	-0.030832	2.844726
153.020708	2656.005080	5.852826	-0.030904	2.848729
153.306963	2664.044711	5.857830	-0.030963	2.852726
153.582104	2672.112204	5.862835	-0.031021	2.856730
153.723682	2680.143562	5.867840	-0.031053	2.860703
153.715562	2688.197292	5.872845	-0.031058	2.864673
154.088074	2696.233461	5.877850	-0.031133	2.868650
154.238123	2704.291929	5.882854	-0.031167	2.872620
154.254112	2712.366443	5.887859	-0.031176	2.876585
154.303562	2720.394218	5.892864	-0.031192	2.880524
154.458377	2728.386184	5.897869	-0.031227	2.884446
154.821904	2736.418305	5.902874	-0.031300	2.888393
155.002753	2744.483180	5.907878	-0.031340	2.892341
155.304701	2752.548965	5.912883	-0.031403	2.896290
155.691893	2760.537586	5.917888	-0.031481	2.900201
156.194930	2768.561038	5.922893	-0.031580	2.904130
156.211907	2776.637636	5.927898	-0.031590	2.908053
156.626441	2784.696231	5.932902	-0.031673	2.911983
156.970668	2792.804636	5.937907	-0.031743	2.915928
156.914248	2800.799547	5.942912	-0.031739	2.919792
157.055719	2808.816356	5.947917	-0.031771	2.923672
157.252327	2816.839819	5.952922	-0.031814	2.927552
157.394732	2824.881900	5.957926	-0.031847	2.931434
157.552051	2832.962977	5.962931	-0.031882	2.935330
158.041044	2840.923249	5.967936	-0.031979	2.939180
158.172379	2848.965582	5.972941	-0.032010	2.943046
158.360290	2857.015051	5.977946	-0.032051	2.946913
158.511770	2865.057597	5.982950	-0.032085	2.950769
158.982865	2873.101766	5.987955	-0.032179	2.954638
159.048675	2881.118565	5.992960	-0.032197	2.958468
159.327548	2889.149109	5.997965	-0.032255	2.962310
159.818879	2897.182534	6.002970	-0.032353	2.966159
159.779856	2905.199358	6.007974	-0.032352	2.969969
160.198253	2913.280862	6.012979	-0.032436	2.973827
160.390638	2921.298388	6.017984	-0.032478	2.977639
160.442373	2929.358432	6.022989	-0.032493	2.981459
160.704460	2937.386668	6.027994	-0.032548	2.985269
160.865396	2945.414880	6.032998	-0.032584	2.989070
161.262436	2953.486667	6.038003	-0.032664	2.992898
161.340599	2961.537082	6.043008	-0.032685	2.996695
161.398372	2969.544805	6.048013	-0.032702	3.000466
161.942967	2977.517336	6.053018	-0.032809	3.004239
161.981185	2985.580725	6.058022	-0.032823	3.008026
161.937213	2993.668263	6.063027	-0.032821	3.011815
162.041628	3001.695711	6.068032	-0.032846	3.015579
162.411757	3009.705464	6.073037	-0.032921	3.019342
162.426617	3017.761827	6.078042	-0.032930	3.023106
162.462875	3025.793867	6.083046	-0.032943	3.026854
162.975112	3033.827303	6.088051	-0.033044	3.030621
162.939022	3041.897037	6.093056	-0.033044	3.034374
163.108924	3049.893563	6.098061	-0.033081	3.038099
163.649903	3057.892590	6.103066	-0.033188	3.041837
163.622566	3065.942880	6.108070	-0.033189	3.045568
163.688100	3074.004941	6.113075	-0.033207	3.049303
163.844729	3082.047297	6.118080	-0.033243	3.053030
164.144986	3090.090918	6.123085	-0.033305	3.056759
164.187803	3098.127552	6.128090	-0.033319	3.060468
164.541480	3106.103536	6.133094	-0.033391	3.064160
164.807469	3114.154625	6.138099	-0.033446	3.067877
165.014793	3122.245391	6.143104	-0.033491	3.071605
165.035075	3130.343339	6.148109	-0.033501	3.075324
165.348797	3138.312317	6.153114	-0.033566	3.078992
165.643045	3146.294987	6.158118	-0.033626	3.082661
166.161235	3154.319335	6.163123	-0.033729	3.086356
166.186049	3162.342478	6.168128	-0.033740	3.090022
166.539979	3170.384487	6.173133	-0.033812	3.093708
166.853516	3178.410174	6.178138	-0.033876	3.097380
167.001184	3186.449150	6.183142	-0.033910	3.101046
167.189754	3194.475078	6.188147	-0.033951	3.104704
167.445336	3202.516953	6.193152	-0.034005	3.108368
167.571861	3210.586143	6.198157	-0.034034	3.112033
168.012278	3218.607485	6.203162	-0.034122	3.115687
168.000053	3226.617845	6.208166	-0.034126	3.119312
168.072636	3234.683028	6.213171	-0.034146	3.122960
168.336733	3242.687540	6.218176	-0.034201	3.126586
168.586847	3250.697324	6.223181	-0.034254	3.130209
168.707481	3258.795172	6.228186	-0.034282	3.133862
168.817651	3266.810518	6.233190	-0.034309	3.137473
169.258094	3274.843072	6.238195	-0.034397	3.141102
169.489963	3282.818575	6.243200	-0.034446	3.144692
169.537727	3290.890297	6.248205	-0.034461	3.148313
169.816927	3298.950860	6.253210	-0.034519	3.151935
170.050559	3306.995249	6.258214	-0.034569	3.155543
170.471444	3314.972045	6.263219	-0.034653	3.159125
170.579596	3322.991239	6.268224	-0.034680	3.162709
170.634046	3331.050018	6.273229	-0.034696	3.166303
170.847839	3339.081554	6.278234	-0.034742	3.169889
170.962129	3347.128378	6.283238	-0.034769	3.173472
171.177203	3355.186625	6.288243	-0.034815	3.177061
171.399298	3363.173875	6.293248	-0.034863	3.180615
171.425537	3371.201627	6.298253	-0.034874	3.184175
171.788732	3379.249915	6.303258	-0.034947	3.187753
171.901021	3387.284756	6.308262	-0.034974	3.191311
172.234588	3395.317460	6.313267	-0.035043	3.194874
172.618660	3403.284419	6.318272	-0.035120	3.198406
172.767679	3411.330157	6.323277	-0.035154	3.201958
173.076687	3419.366227	6.328282	-0.035218	3.205509
173.273426	3427.393559	6.333286	-0.035260	3.209048
173.609622	3435.472182	6.338291	-0.035329	3.212610
173.737084	3443.513372	6.343296	-0.035359	3.216144
173.845394	3451.528216	6.348301	-0.035385	3.219662
174.136274	3459.549059	6.353306	-0.035446	3.223186
174.425610	3467.565405	6.358310	-0.035505	3.226703
174.749828	3475.593119	6.363315	-0.035572	3.230224
174.817707	3483.700144	6.368320	-0.035591	3.233764
175.065781	3491.694021	6.373325	-0.035643	3.237259
175.247900	3499.717844	6.378330	-0.035683	3.240761
175.228802	3507.715908	6.383334	-0.035685	3.244239
175.589915	3515.756484	6.388339	-0.035759	3.247747
175.951629	3523.767740	6.393344	-0.035832	3.251239
176.027409	3531.814070	6.398349	-0.035852	3.254730
176.400305	3539.830301	6.403354	-0.035928	3.258217
176.539684	3547.857183	6.408358	-0.035960	3.261695
176.869090	3555.877527	6.413363	-0.036027	3.265174
177.046380	3563.926245	6.418368	-0.036067	3.268656
177.308897	3571.962852	6.423373	-0.036122	3.272132
177.516148	3580.021859	6.428378	-0.036166	3.275612
177.589659	3588.013090	6.433382	-0.036186	3.279053
178.151631	3596.013690	6.438387	-0.036297	3.282515
178.369051	3604.041709	6.443392	-0.036343	3.285970
178.499656	3612.097753	6.448397	-0.036374	3.289431
178.723103	3620.162769	6.453402	-0.036421	3.292895
179.080539	3628.172584	6.458406	-0.036494	3.296338
179.143762	3636.213591	6.463411	-0.036512	3.299779
179.282748	3644.225561	6.468416	-0.036544	3.303206
179.739370	3652.257933	6.473421	-0.036635	3.306651
179.875622	3660.295107	6.478426	-0.036667	3.310082
179.881455	3668.363252	6.483430	-0.036674	3.313518
180.323063	3676.396126	6.488435	-0.036762	3.316951
180.635906	3684.369508	6.493440	-0.036826	3.320351
180.867527	3692.374558	6.498445	-0.036876	3.323758
181.076264	3700.428256	6.503450	-0.036921	3.327181
181.169886	3708.444399	6.508454	-0.036944	3.330580
181.539016	3716.503756	6.513459	-0.037019	3.334004
181.637273	3724.527968	6.518464	-0.037043	3.337400
181.957540	3732.543308	6.523469	-0.037109	3.340797
182.574149	3740.524949	6.528474	-0.037230	3.344187
182.656051	3748.588738	6.533478	-0.037251	3.347588
182.858035	3756.648172	6.538483	-0.037295	3.350989
183.169267	3764.670084	6.543488	-0.037359	3.354374
183.590076	3772.657373	6.548493	-0.037443	3.357745
183.736547	3780.724080	6.553498	-0.037477	3.361136
183.880096	3788.689752	6.558502	-0.037510	3.364481
184.119843	3796.776015	6.563507	-0.037560	3.367877
184.263496	3804.809333	6.568512	-0.037593	3.371244
184.309239	3812.837419	6.573517	-0.037608	3.374602
184.845602	3820.856575	6.578522	-0.037714	3.377970
184.775310	3828.900177	6.583526	-0.037707	3.381323
185.094892	3836.879081	6.588531	-0.037772	3.384660
185.647017	3844.893682	6.593536	-0.037881	3.388016
186.019522	3852.939117	6.598541	-0.037957	3.391376
186.350530	3861.074377	6.603546	-0.038025	3.394768
186.604969	3869.027200	6.608550	-0.038078	3.398078
186.990394	3877.064342	6.613555	-0.038156	3.401425
186.945576	3885.052695	6.618560	-0.038154	3.404733
187.176430	3893.074948	6.623565	-0.038203	3.408061
187.426186	3901.145899	6.628570	-0.038255	3.411407
187.480845	3909.148786	6.633574	-0.038271	3.414715
187.591405	3917.176048	6.638579	-0.038298	3.418031
187.903079	3925.213549	6.643584	-0.038362	3.421356
188.199188	3933.162470	6.648589	-0.038423	3.424640
188.516566	3941.239645	6.653594	-0.038489	3.427974
188.616501	3949.271190	6.658598	-0.038513	3.431279
188.934313	3957.314063	6.663603	-0.038579	3.434593
189.242592	3965.341275	6.668608	-0.038642	3.437896
189.573942	3973.348578	6.673613	-0.038710	3.441189
189.766185	3981.354383	6.678618	-0.038752	3.444474
189.998518	3989.410503	6.683622	-0.038801	3.447777
190.256906	3997.477718	6.688627	-0.038855	3.451083
190.241205	4005.478437	6.693632	-0.038859	3.454349
190.332552	4013.515667	6.698637	-0.038882	3.457631
190.732673	4021.538185	6.703642	-0.038962	3.460913
190.818052	4029.529185	6.708646	-0.038984	3.464169
191.043655	4037.569577	6.713651	-0.039032	3.467447
191.402486	4045.607112	6.718656	-0.039105	3.470725
191.333435	4053.685546	6.723661	-0.039099	3.474003
191.743604	4061.733720	6.728666	-0.039181	3.477280
191.847344	4069.673544	6.733670	-0.039206	3.480501
191.940626	4077.689500	6.738675	-0.039230	3.483749
192.094425	4085.728321	6.743680	-0.039265	3.487005
192.303385	4093.710900	6.748685	-0.039310	3.490237
192.745126	4101.788046	6.753690	-0.039398	3.493512
192.822238	4109.798365	6.758694	-0.039418	3.496745
193.212277	4117.811998	6.763699	-0.039497	3.499986
193.241282	4125.868973	6.768704	-0.039509	3.503231
193.565508	4133.838402	6.773709	-0.039575	3.506446
193.904244	4141.898919	6.778714	-0.039644	3.509695
193.960150	4149.942127	6.783718	-0.039661	3.512926
194.166836	4158.013145	6.788723	-0.039705	3.516170
194.319473	4165.979705	6.793728	-0.039740	3.519367
194.612408	4173.981896	6.798733	-0.039800	3.522579
194.677565	4182.024486	6.803738	-0.039819	3.525798
194.791568	4190.041055	6.808742	-0.039846	3.529005
195.150323	4198.085567	6.813747	-0.039919	3.532227
195.446273	4206.117284	6.818752	-0.039980	3.535440
195.486554	4214.156110	6.823757	-0.039994	3.538645
195.888023	4222.175120	6.828762	-0.040074	3.541849
196.104120	4230.147158	6.833766	-0.040121	3.545027
196.547530	4238.226577	6.838771	-0.040209	3.548251
196.700233	4246.286451	6.843776	-0.040244	3.551456
196.748200	4254.397689	6.848781	-0.040259	3.554675
197.013639	4262.374092	6.853786	-0.040315	3.557844
197.077369	4270.330055	6.858790	-0.040332	3.560996
197.185216	4278.331697	6.863795	-0.040359	3.564165
197.511820	4286.355245	6.868800	-0.040426	3.567346
197.701993	4294.383466	6.873805	-0.040467	3.570522
197.744158	4302.445594	6.878810	-0.040481	3.573704
197.992459	4310.438091	6.883814	-0.040533	3.576862
198.158523	4318.453274	6.888819	-0.040570	3.580024
198.284287	4326.455534	6.893824	-0.040600	3.583176
198.464876	4334.519728	6.898829	-0.040640	3.586352
198.871315	4342.518400	6.903834	-0.040721	3.589506
199.114564	4350.547191	6.908838	-0.040773	3.592664
199.429095	4358.599555	6.913843	-0.040837	3.595830
199.601198	4366.580870	6.918848	-0.040875	3.598962
199.603034	4374.630856	6.923853	-0.040882	3.602113
199.838707	4382.616139	6.928858	-0.040932	3.605242
199.925883	4390.632612	6.933862	-0.040954	3.608377
200.083280	4398.683934	6.938867	-0.040990	3.611525
200.224572	4406.733087	6.943872	-0.041022	3.614668
200.313347	4414.756954	6.948877	-0.041045	3.617798
200.663115	4422.756649	6.953882	-0.041116	3.620922
200.596009	4430.780580	6.958886	-0.041109	3.624042
200.791396	4438.816370	6.963891	-0.041152	3.627171
201.135839	4446.825489	6.968896	-0.041222	3.630291
201.126938	4454.904040	6.973901	-0.041227	3.633425
201.356748	4462.962564	6.978906	-0.041276	3.636556
201.756255	4470.883375	6.983910	-0.041356	3.639634
202.027183	4478.923238	6.988915	-0.041412	3.642753
202.396982	4486.926175	6.993920	-0.041487	3.645858
202.905036	4494.934724	6.998925	-0.041588	3.648966
203.206343	4503.022714	7.003930	-0.041650	3.652096
203.412061	4511.040885	7.008934	-0.041695	3.655194
203.628108	4519.071743	7.013939	-0.041741	3.658294
203.807806	4527.106301	7.018944	-0.041781	3.661392
203.780174	4535.102484	7.023949	-0.041782	3.664468
204.230395	4543.144720	7.028954	-0.041871	3.667571
204.370344	4551.166007	7.033958	-0.041904	3.670655
204.460131	4559.230028	7.038963	-0.041926	3.673752
204.711392	4567.259985	7.043968	-0.041979	3.676837
204.733294	4575.228087	7.048973	-0.041989	3.679890
205.087788	4583.262363	7.053978	-0.042062	3.682974
205.210068	4591.249480	7.058982	-0.042090	3.686032
205.478440	4599.278614	7.063987	-0.042146	3.689107
205.734644	4607.318649	7.068992	-0.042200	3.692183
205.987416	4615.328892	7.073997	-0.042253	3.695245
205.952052	4623.348345	7.079002	-0.042253	3.698301
206.054055	4631.387616	7.084006	-0.042278	3.701365
206.461368	4639.361233	7.089011	-0.042360	3.704409
206.774973	4647.401067	7.094016	-0.042424	3.707474
206.824071	4655.428609	7.099021	-0.042440	3.710525
207.226904	4663.566732	7.104026	-0.042521	3.713623
207.312107	4671.585640	7.109030	-0.042543	3.716667
207.611908	4679.519955	7.114035	-0.042605	3.719681
207.860249	4687.516098	7.119040	-0.042657	3.722714
208.255528	4695.507058	7.124045	-0.042737	3.725747
208.405814	4703.568999	7.129050	-0.042771	3.728798
208.695627	4711.550238	7.134054	-0.042831	3.731820
209.040505	4719.622340	7.139059	-0.042901	3.734874
209.006450	4727.672009	7.144064	-0.042901	3.737909
209.161571	4735.655020	7.149069	-0.042936	3.740920
209.560955	4743.670772	7.154074	-0.043016	3.743947
209.880460	4751.701489	7.159078	-0.043082	3.746976
209.865888	4759.753765	7.164083	-0.043085	3.750002
210.187513	4767.800071	7.169088	-0.043151	3.753031
210.450646	4775.829167	7.174093	-0.043206	3.756050
210.583621	4783.814536	7.179098	-0.043237	3.759047
210.674452	4791.834772	7.184102	-0.043260	3.762054
210.964445	4799.846806	7.189107	-0.043320	3.765060
211.137773	4807.867471	7.194112	-0.043359	3.768064
211.441250	4815.904275	7.199117	-0.043421	3.771075
211.754873	4823.961247	7.204122	-0.043486	3.774090
211.902772	4831.949424	7.209126	-0.043519	3.777074
212.204265	4839.969107	7.214131	-0.043581	3.780071
212.540329	4847.962204	7.219136	-0.043650	3.783056
212.698427	4856.007637	7.224141	-0.043686	3.786055
212.823108	4864.049759	7.229146	-0.043715	3.789049
213.274359	4872.074732	7.234150	-0.043805	3.792041
213.746763	4880.096591	7.239155	-0.043899	3.795031
214.016873	4888.093139	7.244160	-0.043956	3.798004
214.136051	4896.098204	7.249165	-0.043984	3.800974
214.531680	4904.094254	7.254170	-0.044064	3.803945
214.784272	4912.163300	7.259174	-0.044117	3.806938
214.921352	4920.150956	7.264179	-0.044148	3.809895
215.057732	4928.233660	7.269184	-0.044180	3.812885
215.158994	4936.200484	7.274189	-0.044205	3.815830
215.215072	4944.239593	7.279194	-0.044221	3.818797
215.351964	4952.258331	7.284198	-0.044253	3.821757
215.596495	4960.257702	7.289203	-0.044304	3.824710
216.022444	4968.281029	7.294208	-0.044390	3.827672
216.100901	4976.281254	7.299213	-0.044410	3.830617
216.319461	4984.395308	7.304218	-0.044457	3.833604
216.605748	4992.410784	7.309222	-0.044517	3.836554
216.874697	5000.372263	7.314227	-0.044573	3.839482
216.993606	5008.431809	7.319232	-0.044601	3.842440
217.172641	5016.401368	7.324237	-0.044641	3.845364
217.213782	5024.456398	7.329242	-0.044654	3.848314
217.393207	5032.479242	7.334246	-0.044694	3.851253
217.906155	5040.496719	7.339251	-0.044795	3.854195
217.961861	5048.544857	7.344256	-0.044812	3.857136
218.085487	5056.514164	7.349261	-0.044841	3.860048
218.453346	5064.577245	7.354266	-0.044916	3.862996
218.514380	5072.577666	7.359270	-0.044933	3.865913
218.451859	5080.646610	7.364275	-0.044927	3.868851
218.820766	5088.717231	7.369280	-0.045002	3.871795
219.081935	5096.903034	7.374285	-0.045057	3.874777
219.139387	5104.841454	7.379290	-0.045074	3.877663
219.224026	5112.759423	7.384294	-0.045096	3.880539
219.640768	5120.711244	7.389299	-0.045179	3.883432
219.910786	5128.741581	7.394304	-0.045236	3.886349
219.871445	5136.752190	7.399309	-0.045234	3.889250
219.935273	5144.815104	7.404314	-0.045252	3.892170
220.253912	5152.801661	7.409318	-0.045318	3.895065
220.493416	5160.837326	7.414323	-0.045368	3.897974
220.641355	5168.858800	7.419328	-0.045402	3.900874
220.742190	5176.812608	7.424333	-0.045427	3.903747
221.093714	5184.879739	7.429338	-0.045498	3.906663
221.148773	5192.895530	7.434342	-0.045515	3.909553
221.478614	5200.930069	7.439347	-0.045582	3.912452
221.838135	5208.972674	7.444352	-0.045655	3.915353
221.831358	5216.938433	7.449357	-0.045660	3.918217
222.467883	5224.986046	7.454362	-0.045785	3.921120
222.468808	5232.951981	7.459366	-0.045791	3.923980
222.438236	5241.001930	7.464371	-0.045791	3.926867
222.710687	5249.003401	7.469376	-0.045848	3.929741
223.078447	5257.057530	7.474381	-0.045923	3.932633
223.556333	5265.077376	7.479386	-0.046018	3.935512
223.517143	5273.074803	7.484390	-0.046017	3.938372
223.676666	5281.102302	7.489395	-0.046052	3.941245
224.370345	5289.100723	7.494400	-0.046188	3.944114
224.371096	5297.146213	7.499405	-0.046194	3.946985
224.743126	5305.147934	7.504410	-0.046269	3.949846
224.847309	5313.222969	7.509414	-0.046295	3.952725
225.177382	5321.221105	7.514419	-0.046362	3.955580
225.527769	5329.231208	7.519424	-0.046434	3.958436
225.421696	5337.265652	7.524429	-0.046420	3.961292
225.779762	5345.259940	7.529434	-0.046493	3.964139
225.924651	5353.284357	7.534438	-0.046526	3.966991
226.167969	5361.301150	7.539443	-0.046577	3.969839
226.497700	5369.344397	7.544448	-0.046645	3.972697
226.498148	5377.349131	7.549453	-0.046651	3.975533
226.758496	5385.387994	7.554458	-0.046705	3.978384
227.027780	5393.396136	7.559462	-0.046762	3.981222
227.074148	5401.409866	7.564467	-0.046776	3.984056
227.179064	5409.462867	7.569472	-0.046802	3.986903
227.378881	5417.467770	7.574477	-0.046845	3.989732
227.623408	5425.550759	7.579482	-0.046897	3.992588
227.825122	5433.560102	7.584486	-0.046941	3.995415
227.982480	5441.555065	7.589491	-0.046976	3.998234
228.347819	5449.574720	7.594496	-0.047050	4.001063
228.598954	5457.536116	7.599501	-0.047103	4.003868
228.763998	5465.603020	7.604506	-0.047140	4.006707
228.903079	5473.572867	7.609510	-0.047172	4.009509
229.181832	5481.652461	7.614515	-0.047230	4.012349
229.206545	5489.685949	7.619520	-0.047240	4.015168
229.502241	5497.655241	7.624525	-0.047302	4.017966
229.780024	5505.682718	7.629530	-0.047359	4.020783
229.824140	5513.681554	7.634534	-0.047374	4.023583
230.042988	5521.713207	7.639539	-0.047421	4.026396
230.400709	5529.746349	7.644544	-0.047493	4.029210
230.455859	5537.788479	7.649549	-0.047510	4.032020
230.756331	5545.920559	7.654554	-0.047572	4.034863
230.944850	5553.844834	7.659558	-0.047613	4.037630
231.147706	5561.834947	7.664563	-0.047657	4.040418
231.440830	5569.842989	7.669568	-0.047717	4.043212
231.547290	5577.843934	7.674573	-0.047743	4.045999
231.729986	5585.867901	7.679578	-0.047783	4.048793
231.953429	5593.896693	7.684582	-0.047831	4.051587
231.881418	5601.929924	7.689587	-0.047824	4.054377
232.460929	5609.919221	7.694592	-0.047938	4.057158
232.385674	5617.921406	7.699597	-0.047930	4.059933
232.498606	5625.974486	7.704602	-0.047957	4.062726
232.628545	5633.951331	7.709606	-0.047987	4.065492
232.925607	5641.964777	7.714611	-0.048049	4.068270
233.312990	5650.056022	7.719616	-0.048127	4.071074
233.539648	5658.019448	7.724621	-0.048175	4.073830
233.891618	5666.086418	7.729626	-0.048247	4.076622
233.782387	5674.049876	7.734630	-0.048232	4.079370
234.075907	5682.079660	7.739635	-0.048293	4.082144
234.359788	5690.086430	7.744640	-0.048352	4.084908
234.429857	5698.088100	7.749645	-0.048371	4.087666
234.729428	5706.118004	7.754650	-0.048433	4.090435
234.935800	5714.158917	7.759654	-0.048478	4.093204
235.029961	5722.200623	7.764659	-0.048501	4.095970
235.135602	5730.241009	7.769664	-0.048527	4.098734
235.223957	5738.227503	7.774669	-0.048550	4.101477
235.871816	5746.218123	7.779674	-0.048676	4.104227
235.997403	5754.263300	7.784678	-0.048706	4.106987
236.262699	5762.273142	7.789683	-0.048761	4.109735
236.679204	5770.337525	7.794688	-0.048845	4.112502
236.626082	5778.355659	7.799693	-0.048841	4.115245
236.853451	5786.370557	7.804698	-0.048890	4.117989
237.174408	5794.360948	7.809702	-0.048955	4.120723
237.462596	5802.349760	7.814707	-0.049015	4.123455
237.582456	5810.406880	7.819712	-0.049043	4.126206
237.619180	5818.399192	7.824717	-0.049056	4.128932
238.236166	5826.497743	7.829722	-0.049177	4.131700
238.388326	5834.488464	7.834726	-0.049212	4.134423
238.502679	5842.509733	7.839731	-0.049239	4.137155
238.771197	5850.534558	7.844736	-0.049295	4.139887
238.904857	5858.526384	7.849741	-0.049326	4.142605
238.967152	5866.540740	7.854746	-0.049344	4.145328
239.146564	5874.574710	7.859750	-0.049383	4.148058
239.647992	5882.589982	7.864755	-0.049483	4.150783
239.660881	5890.685650	7.869760	-0.049491	4.153527
239.688607	5898.658959	7.874765	-0.049503	4.156229
240.242783	5906.656397	7.879770	-0.049612	4.158943
240.523888	5914.677800	7.884774	-0.049670	4.161660
240.582429	5922.634492	7.889779	-0.049687	4.164350
240.988099	5930.695630	7.894784	-0.049769	4.167079
241.298390	5938.664593	7.899789	-0.049833	4.169773
241.479846	5946.735674	7.904794	-0.049873	4.172499
241.390155	5954.737706	7.909798	-0.049862	4.175196
241.897469	5962.763310	7.914803	-0.049963	4.177906
242.186922	5970.802370	7.919808	-0.050023	4.180617
242.256053	5978.757405	7.924813	-0.050042	4.183295
242.260282	5986.849662	7.929818	-0.050048	4.186017
242.589064	5994.819737	7.934822	-0.050116	4.188699
242.789967	6002.836322	7.939827	-0.050159	4.191394
243.108232	6010.981911	7.944832	-0.050225	4.194132
243.102933	6018.982066	7.949837	-0.050230	4.196815
243.210741	6026.912087	7.954842	-0.050256	4.199475
243.498958	6034.915231	7.959846	-0.050316	4.202159
243.870413	6042.886541	7.964851	-0.050391	4.204832
243.986848	6050.956768	7.969856	-0.050419	4.207533
243.950643	6058.924807	7.974861	-0.050418	4.210197
244.419698	6067.005035	7.979866	-0.050511	4.212902
244.591457	6075.009814	7.984870	-0.050549	4.215577
244.763490	6083.011326	7.989875	-0.050588	4.218249
245.116623	6091.015429	7.994880	-0.050659	4.220922
245.281525	6099.003134	7.999885	-0.050696	4.223586
245.581295	6107.081080	8.004890	-0.050758	4.226280
245.416960	6115.039894	8.009894	-0.050734	4.228928
245.783103	6123.121622	8.014899	-0.050808	4.231620
246.141689	6131.161905	8.019904	-0.050881	4.234296
246.230608	6139.167175	8.024909	-0.050903	4.236957
246.277587	6147.141086	8.029914	-0.050918	4.239605
246.455831	6155.201967	8.034918	-0.050957	4.242282
246.661561	6163.111865	8.039923	-0.051002	4.244907
246.788124	6171.252281	8.044928	-0.051031	4.247606
247.036656	6179.223905	8.049933	-0.051084	4.250248
247.176236	6187.320577	8.054938	-0.051116	4.252929
247.246220	6195.301575	8.059942	-0.051135	4.255570
247.595937	6203.308375	8.064947	-0.051206	4.258220
247.883176	6211.336165	8.069952	-0.051266	4.260874
247.788507	6219.330981	8.074957	-0.051254	4.263513
248.183980	6227.341471	8.079962	-0.051334	4.266160
248.393422	6235.388489	8.084966	-0.051379	4.268815
248.460940	6243.422498	8.089971	-0.051398	4.271463
248.599006	6251.465402	8.094976	-0.051430	4.274113
248.790696	6259.464547	8.099981	-0.051471	4.276747
249.005953	6267.444378	8.104986	-0.051517	4.279374
249.229677	6275.512599	8.109990	-0.051565	4.282028
249.319573	6283.425757	8.114995	-0.051588	4.284628
249.603559	6291.552034	8.120000	-0.051647	4.287298
249.667034	6299.513786	8.125005	-0.051665	4.289911
249.878745	6307.578720	8.130010	-0.051710	4.292557
250.054541	6315.575260	8.135014	-0.051749	4.295179
250.185748	6323.549229	8.140019	-0.051780	4.297792
250.332791	6331.609794	8.145024	-0.051813	4.300431
250.691717	6339.597814	8.150029	-0.051886	4.303047
251.039318	6347.662767	8.155034	-0.051957	4.305686
251.145025	6355.617029	8.160038	-0.051983	4.308285
251.241585	6363.639488	8.165043	-0.052007	4.310905
251.484310	6371.758294	8.170048	-0.052058	4.313556
251.435954	6379.747050	8.175053	-0.052055	4.316161
251.759576	6387.716940	8.180058	-0.052121	4.318760
251.956789	6395.747323	8.185062	-0.052164	4.321377
252.047740	6403.695776	8.190067	-0.052187	4.323965
252.139866	6411.765175	8.195072	-0.052211	4.326591
252.132061	6419.755231	8.200077	-0.052215	4.329188
252.398612	6427.773038	8.205082	-0.052271	4.331795
252.795736	6435.850721	8.210086	-0.052351	4.334421
252.797905	6443.858070	8.215091	-0.052357	4.337019
253.005572	6451.820681	8.220096	-0.052402	4.339603
252.991181	6459.836083	8.225101	-0.052406	4.342201
253.336070	6467.852782	8.230106	-0.052476	4.344800
253.486479	6475.879342	8.235110	-0.052510	4.347399
253.510837	6483.849601	8.240115	-0.052521	4.349978
253.856600	6492.005587	8.245120	-0.052591	4.352617
254.030017	6500.023170	8.250125	-0.052629	4.355209
254.111057	6507.973916	8.255130	-0.052651	4.357777
254.339469	6515.960412	8.260134	-0.052699	4.360356
254.451374	6523.954934	8.265139	-0.052726	4.362936
254.755917	6532.016470	8.270144	-0.052789	4.365536
254.704036	6539.994629	8.275149	-0.052785	4.368106
254.902188	6548.003874	8.280154	-0.052828	4.370686
255.094256	6556.074342	8.285158	-0.052870	4.373285
255.326505	6564.049916	8.290163	-0.052920	4.375851
255.331202	6572.068369	8.295168	-0.052926	4.378428
255.421294	6580.090041	8.300173	-0.052949	4.381005
255.841230	6588.109712	8.305178	-0.053034	4.383582
255.916444	6596.138324	8.310182	-0.053054	4.386158
256.136871	6604.138034	8.315187	-0.053101	4.388725
256.414118	6612.213674	8.320192	-0.053159	4.391314
256.658948	6620.209911	8.325197	-0.053210	4.393876
256.814714	6628.240696	8.330202	-0.053245	4.396448
256.969430	6636.219647	8.335206	-0.053280	4.399001
257.038736	6644.259392	8.340211	-0.053299	4.401571
257.263164	6652.238836	8.345216	-0.053347	4.404122
257.416498	6660.290632	8.350221	-0.053382	4.406694
257.557913	6668.274975	8.355226	-0.053414	4.409243
257.612941	6676.344646	8.360230	-0.053430	4.411817
257.840092	6684.346881	8.365235	-0.053479	4.414369
258.025465	6692.436819	8.370240	-0.053519	4.416947
258.117365	6700.376017	8.375245	-0.053543	4.419475
258.119674	6708.410428	8.380250	-0.053549	4.422032
258.326415	6716.375841	8.385254	-0.053594	4.424566
258.810641	6724.433335	8.390259	-0.053690	4.427129
258.960827	6732.441409	8.395264	-0.053724	4.429674
258.961176	6740.504436	8.400269	-0.053730	4.432233
259.238168	6748.526029	8.405274	-0.053788	4.434780
259.470209	6756.560836	8.410278	-0.053837	4.437328
259.703855	6764.488990	8.415283	-0.053887	4.439842
260.096307	6772.576433	8.420288	-0.053966	4.442405
260.094068	6780.540614	8.425293	-0.053972	4.444926
260.407296	6788.553689	8.430298	-0.054036	4.447462
260.470271	6796.560772	8.435302	-0.054054	4.449994
260.501895	6804.580742	8.440307	-0.054066	4.452529
260.779762	6812.681428	8.445312	-0.054124	4.455088
260.794585	6820.643595	8.450317	-0.054132	4.457601
261.189835	6828.635511	8.455322	-0.054212	4.460124
261.535966	6836.656456	8.460326	-0.054283	4.462654
261.696560	6844.647531	8.465331	-0.054319	4.465173
262.013669	6852.696982	8.470336	-0.054384	4.467709
261.888518	6860.695452	8.475341	-0.054367	4.470226
262.086091	6868.742578	8.480346	-0.054409	4.472757
262.437066	6876.771872	8.485350	-0.054481	4.475283
262.591451	6884.763159	8.490355	-0.054516	4.477794
262.724226	6892.798007	8.495360	-0.054547	4.480318
262.677902	6900.752661	8.500365	-0.054544	4.482814
263.101968	6908.782812	8.505370	-0.054629	4.485334
263.284877	6916.827934	8.510374	-0.054669	4.487857
263.196547	6924.845323	8.515379	-0.054659	4.490368
263.428644	6932.894152	8.520384	-0.054708	4.492889
263.418077	6940.849996	8.525389	-0.054712	4.495379
263.801178	6948.884672	8.530394	-0.054790	4.497893
263.941930	6956.886128	8.535398	-0.054822	4.500395
264.174150	6964.892332	8.540403	-0.054871	4.502897
264.301654	6972.928953	8.545408	-0.054901	4.505407
264.373865	6980.939537	8.550413	-0.054921	4.507907
264.844527	6989.002554	8.555418	-0.055014	4.510423
265.137471	6997.039566	8.560423	-0.055075	4.512929
265.143261	7005.045213	8.565427	-0.055082	4.515423
265.440734	7013.031124	8.570432	-0.055144	4.517910
265.524819	7021.010018	8.575437	-0.055165	4.520394
265.534665	7029.001882	8.580442	-0.055173	4.522879
265.728759	7037.025060	8.585447	-0.055215	4.525374
265.973464	7045.012218	8.590451	-0.055267	4.527856
266.171230	7053.086627	8.595456	-0.055310	4.530363
266.101167	7061.109863	8.600461	-0.055303	4.532853
266.531778	7069.133547	8.605466	-0.055389	4.535343
266.836178	7077.153468	8.610471	-0.055452	4.537829
266.884477	7085.057359	8.615475	-0.055467	4.540278
267.250712	7093.150437	8.620480	-0.055541	4.542785
267.434325	7101.121926	8.625485	-0.055582	4.545252
267.543418	7109.216318	8.630490	-0.055608	4.547756
267.671564	7117.219167	8.635495	-0.055638	4.550230
267.719597	7125.281372	8.640499	-0.055653	4.552721
267.940577	7133.287610	8.645504	-0.055700	4.555194
267.940244	7141.291109	8.650509	-0.055706	4.557664
268.339735	7149.253861	8.655514	-0.055787	4.560121
268.537518	7157.316027	8.660519	-0.055830	4.562607
268.563293	7165.277879	8.665523	-0.055841	4.565060
268.772867	7173.324546	8.670528	-0.055886	4.567538
268.867858	7181.309069	8.675533	-0.055909	4.569996
269.014224	7189.383060	8.680538	-0.055943	4.572480
269.202474	7197.421779	8.685543	-0.055984	4.574951
269.411361	7205.402885	8.690547	-0.056029	4.577404
269.495903	7213.400856	8.695552	-0.056051	4.579860
269.421825	7221.448272	8.700557	-0.056043	4.582330
269.727847	7229.416810	8.705562	-0.056106	4.584775
270.095391	7237.487396	8.710567	-0.056181	4.587250
270.313347	7245.482226	8.715571	-0.056227	4.589700
270.364716	7253.541808	8.720576	-0.056243	4.592169
270.527106	7261.581142	8.725581	-0.056279	4.594630
270.839246	7269.575718	8.730586	-0.056344	4.597076
271.134628	7277.567548	8.735591	-0.056405	4.599520
271.251635	7285.579187	8.740595	-0.056432	4.601968
271.326511	7293.554272	8.745600	-0.056452	4.604405
271.542375	7301.592916	8.750605	-0.056499	4.606859
271.697464	7309.555090	8.755610	-0.056534	4.609288
271.922348	7317.636233	8.760615	-0.056582	4.611753
271.913239	7325.646918	8.765619	-0.056586	4.614195
271.999279	7333.688558	8.770624	-0.056608	4.616644
272.280952	7341.652613	8.775629	-0.056667	4.619069
272.396635	7349.690592	8.780634	-0.056694	4.621515
272.546213	7357.692881	8.785639	-0.056728	4.623949
272.741528	7365.689243	8.790643	-0.056771	4.626380
273.052010	7373.768188	8.795648	-0.056835	4.628835
273.162717	7381.760709	8.800653	-0.056861	4.631262
273.340244	7389.801846	8.805658	-0.056900	4.633702
273.669229	7397.818800	8.810663	-0.056968	4.636134
273.793501	7405.753105	8.815667	-0.056997	4.638539
273.906275	7413.821404	8.820672	-0.057024	4.640984
274.175392	7421.809887	8.825677	-0.057080	4.643403
274.495371	7429.832715	8.830682	-0.057146	4.645832
274.531299	7437.865186	8.835687	-0.057159	4.648262
274.513338	7445.867625	8.840691	-0.057161	4.650682
274.763148	7453.938201	8.845696	-0.057214	4.653121
274.792804	7461.914093	8.850701	-0.057226	4.655530
275.076490	7469.894091	8.855706	-0.057285	4.657939
275.316665	7477.970266	8.860711	-0.057335	4.660376
275.102137	7485.943213	8.865715	-0.057302	4.662780
275.416355	7493.927746	8.870720	-0.057366	4.665187
275.719860	7501.941359	8.875725	-0.057429	4.667601
275.875408	7509.959565	8.880730	-0.057464	4.670015
275.992102	7518.098005	8.885735	-0.057492	4.672464
276.172262	7526.127946	8.890739	-0.057531	4.674879
276.679530	7534.158709	8.895744	-0.057632	4.677293
276.881710	7542.005042	8.900749	-0.057675	4.679650
276.813306	7550.092984	8.905754	-0.057669	4.682080
277.099500	7558.022880	8.910759	-0.057728	4.684460
277.285331	7566.079122	8.915763	-0.057769	4.686876
277.392880	7574.068288	8.920768	-0.057795	4.689272
277.556727	7582.118226	8.925773	-0.057832	4.691684
277.770852	7590.144576	8.930778	-0.057878	4.694088
278.098792	7598.190533	8.935783	-0.057945	4.696496
277.989571	7606.143689	8.940787	-0.057930	4.698877
278.372500	7614.227687	8.945792	-0.058008	4.701294
278.398381	7622.174357	8.950797	-0.058019	4.703669
278.515443	7630.155038	8.955802	-0.058047	4.706054
278.611167	7638.236898	8.960807	-0.058071	4.708467
278.846661	7646.198549	8.965811	-0.058120	4.710843
279.048002	7654.284410	8.970816	-0.058164	4.713254
279.187986	7662.280765	8.975821	-0.058196	4.715638
279.380824	7670.311032	8.980826	-0.058238	4.718031
279.538537	7678.309500	8.985831	-0.058274	4.720413
279.622184	7686.338673	8.990835	-0.058295	4.722803
279.865320	7694.332518	8.995840	-0.058347	4.725181
279.975651	7702.350225	9.000845	-0.058373	4.727566
280.055782	7710.395899	9.005850	-0.058394	4.729957
280.383281	7718.440786	9.010855	-0.058461	4.732346
280.621819	7726.445858	9.015859	-0.058512	4.734723
280.588871	7734.478554	9.020864	-0.058512	4.737107
280.703365	7742.400000	9.025869	-0.058539	4.739457
280.855290	7750.442734	9.030874	-0.058574	4.741841
281.078743	7758.446109	9.035879	-0.058621	4.744212
281.015220	7766.509434	9.040883	-0.058616	4.746601
281.373578	7774.502465	9.045888	-0.058688	4.748966
281.522294	7782.548928	9.050893	-0.058722	4.751347
281.631175	7790.584246	9.055898	-0.058748	4.753723
281.916080	7798.620447	9.060903	-0.058808	4.756097
282.130787	7806.562699	9.065907	-0.058854	4.758443
282.439589	7814.612688	9.070912	-0.058917	4.760819
282.231595	7822.567282	9.075917	-0.058885	4.763168
282.528603	7830.536360	9.080922	-0.058946	4.765518
282.781610	7838.606360	9.085927	-0.058999	4.767897
282.785497	7846.631684	9.090931	-0.059006	4.770262
282.976411	7854.695283	9.095936	-0.059048	4.772636
283.181796	7862.696356	9.100941	-0.059092	4.774991
283.178652	7870.664666	9.105946	-0.059097	4.777336
283.462248	7878.692888	9.110951	-0.059156	4.779697
283.639069	7886.688647	9.115955	-0.059195	4.782047
283.860945	7894.678429	9.120960	-0.059243	4.784393
283.912806	7902.732509	9.125965	-0.059258	4.786759
284.326742	7910.752278	9.130970	-0.059342	4.789111
284.637853	7918.823596	9.135975	-0.059406	4.791478
284.504203	7926.817819	9.140979	-0.059387	4.793823
284.605657	7934.864234	9.145984	-0.059412	4.796181
284.943804	7942.830899	9.150989	-0.059481	4.798513
284.909309	7950.819229	9.155994	-0.059481	4.800853
285.255165	7958.874005	9.160999	-0.059551	4.803208
285.376943	7966.809738	9.166003	-0.059580	4.805529
285.496142	7974.891366	9.171008	-0.059608	4.807892
285.494240	7982.871394	9.176013	-0.059614	4.810224
285.715622	7990.268894	9.181018	-0.059661	4.812384
285.960103	7994.802027	9.186023	-0.059710	4.813706
286.144417	7997.310792	9.191027	-0.059747	4.814438
286.289665	7998.690860	9.196032	-0.059776	4.814840
286.354313	7999.094188	9.201037	-0.059789	4.814957
286.482308	8000.044115	9.206042	-0.059814	4.815234
286.682124	8000.055036	9.211047	-0.059852	4.815236
286.685498	8000.000617	9.216051	-0.059854	4.815220
286.620049	8000.035964	9.221056	-0.059842	4.815231
286.689192	8000.053248	9.226061	-0.059856	4.815235
286.781908	8000.019584	9.231066	-0.059874	4.815225
286.956710	8000.036503	9.236071	-0.059908	4.815229
287.072921	8000.011791	9.241075	-0.059930	4.815221
287.049350	8000.066026	9.246080	-0.059927	4.815237
287.245476	8000.030890	9.251085	-0.059964	4.815226
287.110004	7999.997671	9.256090	-0.059940	4.815217
287.053720	8000.049218	9.261095	-0.059930	4.815232
286.957269	8000.042327	9.266099	-0.059913	4.815231
287.396416	8000.065827	9.271104	-0.059996	4.815235
287.010217	8000.004863	9.276109	-0.059924	4.815219
287.245927	8000.015318	9.281114	-0.059969	4.815221
287.376138	8000.025071	9.286119	-0.059994	4.815223
287.236994	8000.007835	9.291123	-0.059969	4.815219
287.361319	8000.037814	9.296128	-0.059993	4.815227
287.367152	8000.029432	9.301133	-0.059995	4.815225
287.543836	8000.002526	9.306138	-0.060029	4.815216
287.434729	7999.996492	9.311143	-0.060009	4.815215
287.512670	7999.992530	9.316147	-0.060025	4.815213
287.649045	8000.037687	9.321152	-0.060051	4.815226
287.632539	8000.011815	9.326157	-0.060049	4.815218
287.649165	8000.011102	9.331162	-0.060053	4.815218
287.700573	8000.020601	9.336167	-0.060063	4.815220
287.693285	7999.995953	9.341171	-0.060063	4.815213
287.671210	8000.034169	9.346176	-0.060060	4.815224
287.593558	8000.008339	9.351181	-0.060046	4.815217
287.683273	8000.008854	9.356186	-0.060064	4.815217
287.740316	8000.024866	9.361191	-0.060075	4.815221
287.732583	8000.007699	9.366195	-0.060074	4.815216
287.910884	8000.042864	9.371200	-0.060109	4.815226
287.737647	7999.983336	9.376205	-0.060077	4.815209
287.804832	8000.005937	9.381210	-0.060090	4.815215
287.833853	8000.094218	9.386215	-0.060097	4.815241
287.661177	8000.024003	9.391219	-0.060065	4.815221
287.819520	8000.042787	9.396224	-0.060096	4.815226
288.019239	7999.999153	9.401229	-0.060134	4.815212
287.930801	8000.015930	9.406234	-0.060118	4.815217
287.753241	8000.008745	9.411239	-0.060086	4.815216
287.695243	8000.003569	9.416243	-0.060076	4.815215
288.013784	8000.053928	9.421248	-0.060136	4.815228
287.885605	8000.017620	9.426253	-0.060113	4.815218
287.740121	8000.015254	9.431258	-0.060087	4.815218
287.904388	8000.040555	9.436263	-0.060118	4.815225
287.932994	7999.992977	9.441267	-0.060125	4.815211
288.022424	8000.029858	9.446272	-0.060142	4.815221
287.894522	8000.026716	9.451277	-0.060119	4.815221
288.010905	8000.050144	9.456282	-0.060142	4.815227
288.345852	8000.061200	9.461287	-0.060205	4.815228
288.103366	8000.018692	9.466291	-0.060161	4.815217
288.317369	8000.033064	9.471296	-0.060201	4.815220
288.067615	8000.008619	9.476301	-0.060156	4.815214
288.070978	8000.009823	9.481306	-0.060157	4.815215
288.110687	8000.053357	9.486311	-0.060166	4.815227
288.145785	8000.014445	9.491315	-0.060173	4.815216
288.135656	8000.037886	9.496320	-0.060172	4.815222
288.260235	8000.032570	9.501325	-0.060196	4.815220
288.269309	8000.033869	9.506330	-0.060198	4.815221
288.302630	8000.038786	9.511335	-0.060206	4.815222
288.169339	8000.010950	9.516339	-0.060182	4.815214
288.199340	8000.043624	9.521344	-0.060188	4.815224
288.312542	8000.047744	9.526349	-0.060210	4.815224
288.185703	8000.047829	9.531354	-0.060187	4.815225
288.375396	8000.039328	9.536359	-0.060223	4.815222
288.479089	8000.043288	9.541363	-0.060244	4.815222
288.246381	8000.058709	9.546368	-0.060201	4.815228
288.267468	8000.025980	9.551373	-0.060206	4.815218
288.407458	8000.033759	9.556378	-0.060233	4.815220
288.552860	8000.052327	9.561383	-0.060261	4.815224
288.564909	8000.011957	9.566387	-0.060264	4.815212
288.613955	8000.029975	9.571392	-0.060274	4.815217
288.664480	8000.014856	9.576397	-0.060284	4.815213
288.554167	8000.023777	9.581402	-0.060264	4.815216
288.679154	8000.074094	9.586407	-0.060289	4.815230
288.737320	8000.038778	9.591411	-0.060300	4.815219
288.688039	8000.065841	9.596416	-0.060292	4.815227
288.486629	8000.046487	9.601421	-0.060255	4.815223
288.488045	8000.042309	9.606426	-0.060256	4.815222
288.676406	8000.077646	9.611431	-0.060292	4.815231
288.486306	8000.053133	9.616435	-0.060258	4.815225
288.421104	8000.062812	9.621440	-0.060247	4.815228
288.517372	8000.069857	9.626445	-0.060265	4.815229
288.477375	8000.033961	9.631450	-0.060259	4.815219
288.534490	8000.052114	9.636455	-0.060270	4.815224
288.563054	8000.046254	9.641459	-0.060276	4.815222
288.623369	8000.070880	9.646464	-0.060289	4.815229
288.610508	8000.021533	9.651469	-0.060287	4.815215
288.821847	8000.033722	9.656474	-0.060327	4.815217
288.698159	8000.039208	9.661479	-0.060305	4.815219
288.780782	7999.992537	9.666483	-0.060321	4.815205
288.725857	8000.082619	9.671488	-0.060312	4.815232
288.751323	8000.018940	9.676493	-0.060317	4.815213
288.673168	8000.031611	9.681498	-0.060304	4.815217
288.747409	8000.044704	9.686503	-0.060319	4.815221
288.743747	8000.039371	9.691507	-0.060319	4.815219
288.785215	8000.089354	9.696512	-0.060327	4.815233
288.709257	8000.050714	9.701517	-0.060314	4.815222
288.776750	8000.030531	9.706522	-0.060327	4.815216
288.828767	8000.067855	9.711527	-0.060338	4.815227
288.932670	8000.041866	9.716531	-0.060358	4.815219
288.891573	8000.155716	9.721536	-0.060351	4.815252
288.966228	8000.050074	9.726541	-0.060366	4.815221
288.913669	8000.033222	9.731546	-0.060357	4.815216
288.860794	8000.046317	9.736551	-0.060348	4.815220
288.915978	8000.024858	9.741555	-0.060359	4.815214
288.889162	8000.062996	9.746560	-0.060355	4.815225
288.643872	8000.035416	9.751565	-0.060310	4.815218
288.843232	8000.064519	9.756570	-0.060348	4.815226
289.001713	8000.081168	9.761575	-0.060379	4.815230
288.862614	8000.036117	9.766579	-0.060354	4.815217
288.866467	8000.069422	9.771584	-0.060355	4.815227
288.907741	8000.017776	9.776589	-0.060364	4.815212
288.769981	8000.031584	9.781594	-0.060339	4.815216
288.881305	8000.026045	9.786599	-0.060361	4.815214
288.790906	8000.011766	9.791603	-0.060345	4.815210
288.953455	8000.071273	9.796608	-0.060376	4.815227
288.928136	8000.025996	9.801613	-0.060372	4.815214
289.073055	8000.047765	9.806618	-0.060400	4.815219
289.146734	8000.101500	9.811623	-0.060414	4.815235
288.760996	8000.043744	9.816627	-0.060343	4.815220
288.769568	8000.061082	9.821632	-0.060346	4.815225
288.885457	8000.060968	9.826637	-0.060368	4.815224
288.749135	8000.053405	9.831642	-0.060344	4.815222
289.043555	8000.071270	9.836647	-0.060399	4.815226
288.902588	8000.050792	9.841651	-0.060374	4.815221
289.045445	8000.107829	9.846656	-0.060402	4.815237
288.880449	8000.111551	9.851661	-0.060372	4.815239
288.940393	8000.062358	9.856666	-0.060384	4.815224
288.974795	8000.095107	9.861671	-0.060391	4.815233
288.808549	8000.059227	9.866675	-0.060361	4.815224
288.923300	8000.084769	9.871680	-0.060383	4.815231
288.935057	8000.097881	9.876685	-0.060386	4.815234
288.951574	8000.045819	9.881690	-0.060390	4.815219
288.821805	8000.097202	9.886695	-0.060367	4.815235
289.013968	8000.056651	9.891699	-0.060403	4.815222
289.088556	8000.082588	9.896704	-0.060418	4.815229
288.966343	8000.070983	9.901709	-0.060396	4.815226
288.818812	8000.054673	9.906714	-0.060370	4.815222
289.165095	8000.075550	9.911719	-0.060435	4.815227
289.015659	8000.079533	9.916723	-0.060408	4.815228
288.924388	8000.089844	9.921728	-0.060392	4.815232
288.904828	8000.060709	9.926733	-0.060389	4.815223
288.839743	8000.052204	9.931738	-0.060378	4.815221
289.002880	8000.071071	9.936743	-0.060409	4.815226
288.859271	8000.064455	9.941747	-0.060383	4.815225
288.912452	8000.083613	9.946752	-0.060394	4.815230
288.901639	8000.048207	9.951757	-0.060393	4.815220
288.881881	8000.038325	9.956762	-0.060390	4.815217
289.146246	8000.065313	9.961767	-0.060440	4.815223
289.084286	8000.024768	9.966771	-0.060429	4.815212
289.265098	8000.068537	9.971776	-0.060464	4.815224
289.064732	8000.102687	9.976781	-0.060428	4.815235
288.954146	8000.077370	9.981786	-0.060408	4.815228
289.099192	8000.100213	9.986791	-0.060436	4.815234
288.956426	8000.047611	9.991795	-0.060410	4.815219
289.015431	8000.072216	9.996800	-0.060422	4.815226
288.864835	8000.018413	10.001805	-0.060395	4.815211
288.965934	8000.022330	10.006810	-0.060414	4.815212
289.286948	8000.069526	10.011815	-0.060475	4.815224
289.165700	8000.036542	10.016819	-0.060453	4.815215
289.000834	8000.040266	10.021824	-0.060423	4.815217
289.162422	8000.082642	10.026829	-0.060454	4.815228
289.121995	8000.049947	10.031834	-0.060448	4.815219
289.239493	8000.084094	10.036839	-0.060470	4.815228
289.195627	8000.045992	10.041843	-0.060463	4.815217
289.321116	8000.087762	10.046848	-0.060487	4.815229
289.315444	8000.087744	10.051853	-0.060487	4.815229
289.000632	8000.027970	10.056858	-0.060429	4.815213
289.118610	8000.052496	10.061863	-0.060452	4.815219
289.314534	8000.030195	10.066867	-0.060490	4.815212
289.142468	8000.055193	10.071872	-0.060458	4.815220
289.178191	8000.047313	10.076877	-0.060466	4.815217
289.353162	8000.046054	10.081882	-0.060499	4.815216
289.410722	8000.086682	10.086887	-0.060511	4.815228
289.238158	8000.044276	10.091891	-0.060480	4.815216
289.333015	8000.057716	10.096896	-0.060498	4.815220
289.359783	8000.071081	10.101901	-0.060504	4.815223
289.238254	8000.065906	10.106906	-0.060482	4.815222
289.391601	8000.067493	10.111911	-0.060512	4.815222
289.352963	8000.017712	10.116915	-0.060505	4.815208
289.283746	8000.059416	10.121920	-0.060493	4.815220
289.398508	8000.141657	10.126925	-0.060516	4.815244
289.512646	8000.065561	10.131930	-0.060538	4.815221
289.480523	8000.085424	10.136935	-0.060533	4.815227
289.216814	8000.073578	10.141939	-0.060484	4.815225
289.443246	8000.069976	10.146944	-0.060527	4.815222
289.497816	8000.089157	10.151949	-0.060538	4.815228
289.364398	8000.045270	10.156954	-0.060514	4.815216
289.385604	8000.098123	10.161959	-0.060519	4.815231
289.176126	8000.048678	10.166963	-0.060481	4.815217
289.226777	8000.079561	10.171968	-0.060491	4.815226
289.238841	8000.079842	10.176973	-0.060494	4.815226
289.268588	8000.028001	10.181978	-0.060501	4.815211
289.234392	8000.071364	10.186983	-0.060495	4.815224
289.116044	8000.070521	10.191987	-0.060474	4.815224
289.221676	8000.074515	10.196992	-0.060495	4.815225
289.323452	8000.049560	10.201997	-0.060514	4.815217
289.279601	8000.044622	10.207002	-0.060507	4.815216
289.389113	8000.085053	10.212007	-0.060528	4.815227
289.507338	8000.061445	10.217011	-0.060551	4.815219
289.445216	8000.074385	10.222016	-0.060541	4.815223
289.463806	8000.073705	10.227021	-0.060545	4.815223
289.418671	8000.038791	10.232026	-0.060537	4.815213
289.382709	8000.070357	10.237031	-0.060532	4.815222
289.099921	8000.075307	10.242035	-0.060480	4.815225
289.158038	8000.076362	10.247040	-0.060491	4.815225
289.514208	8000.101686	10.252045	-0.060559	4.815231
289.159266	8000.062631	10.257050	-0.060493	4.815221
289.388606	8000.081543	10.262055	-0.060537	4.815226
289.182428	8000.062106	10.267059	-0.060499	4.815221
289.436977	8000.056838	10.272064	-0.060548	4.815218
289.697435	8000.062366	10.277069	-0.060597	4.815218
289.634258	8000.054963	10.282074	-0.060586	4.815217
289.602416	8000.099436	10.287079	-0.060581	4.815230
289.493174	8000.079489	10.292083	-0.060562	4.815224
289.509029	8000.074485	10.297088	-0.060565	4.815223
289.702577	8000.094935	10.302093	-0.060602	4.815228
289.420387	8000.063522	10.307098	-0.060551	4.815220
289.610177	8000.094606	10.312103	-0.060587	4.815228
289.658501	8000.071962	10.317107	-0.060597	4.815221
289.570557	8000.097304	10.322112	-0.060581	4.815229
289.463968	8000.075263	10.327117	-0.060562	4.815223
289.288590	8000.080949	10.332122	-0.060530	4.815226
289.291470	8000.100332	10.337127	-0.060532	4.815231
289.171798	8000.103745	10.342131	-0.060510	4.815233
289.202940	8000.102207	10.347136	-0.060517	4.815232
289.491208	8000.118902	10.352141	-0.060572	4.815236
289.464097	8000.061825	10.357146	-0.060567	4.815219
289.623443	8000.085979	10.362151	-0.060598	4.815225
289.477330	8000.061134	10.367155	-0.060572	4.815219
289.533435	8000.091039	10.372160	-0.060583	4.815227
289.453447	8000.118655	10.377165	-0.060569	4.815236
289.522189	8000.078168	10.382170	-0.060582	4.815223
289.651791	8000.090054	10.387175	-0.060607	4.815226
289.521265	8000.072959	10.392179	-0.060584	4.815222
289.497615	8000.089756	10.397184	-0.060580	4.815227
289.510809	8000.081497	10.402189	-0.060584	4.815224
289.261654	8000.058128	10.407194	-0.060538	4.815219
289.316269	8000.101915	10.412199	-0.060549	4.815231
289.349743	8000.070463	10.417203	-0.060556	4.815222
289.364243	8000.085761	10.422208	-0.060560	4.815226
289.358710	8000.068630	10.427213	-0.060560	4.815221
289.300757	8000.043128	10.432218	-0.060550	4.815214
289.501315	8000.119324	10.437223	-0.060588	4.815235
289.456936	8000.085492	10.442227	-0.060581	4.815226
289.600474	8000.105101	10.447232	-0.060608	4.815231
289.783400	8000.091140	10.452237	-0.060643	4.815226
289.723180	8000.047413	10.457242	-0.060633	4.815213
289.658124	8000.090258	10.462247	-0.060622	4.815226
289.697403	8000.062112	10.467251	-0.060630	4.815217
289.960694	8000.104062	10.472256	-0.060680	4.815228
289.742540	8000.145401	10.477261	-0.060640	4.815242
289.631520	8000.131843	10.482266	-0.060620	4.815238
289.672374	8000.117631	10.487271	-0.060629	4.815234
289.801179	8000.087782	10.492275	-0.060653	4.815224
289.798138	8000.084599	10.497280	-0.060654	4.815223
289.804656	8000.127578	10.502285	-0.060656	4.815236
289.633784	8000.065943	10.507290	-0.060625	4.815219
289.493386	8000.085055	10.512295	-0.060599	4.815225
289.544214	8000.118081	10.517299	-0.060610	4.815234
289.862683	8000.113889	10.522304	-0.060670	4.815232
289.762216	8000.153998	10.527309	-0.060652	4.815244
289.572090	8000.077062	10.532314	-0.060618	4.815222
289.946227	8000.103760	10.537319	-0.060688	4.815228
289.753735	8000.051389	10.542323	-0.060653	4.815214
289.568709	8000.066540	10.547328	-0.060620	4.815219
289.995812	8000.110177	10.552333	-0.060700	4.815230
289.901405	8000.073363	10.557338	-0.060683	4.815219
289.752280	8000.093397	10.562343	-0.060656	4.815226
289.662928	8000.079135	10.567347	-0.060641	4.815222
289.722307	8000.116584	10.572352	-0.060652	4.815233
289.761668	8000.147278	10.577357	-0.060661	4.815242
289.724419	8000.090031	10.582362	-0.060655	4.815225
289.725566	8000.095477	10.587367	-0.060656	4.815227
289.661880	8000.053831	10.592371	-0.060645	4.815215
289.595709	8000.078470	10.597376	-0.060633	4.815222
289.816393	8000.100447	10.602381	-0.060675	4.815227
289.919809	8000.063753	10.607386	-0.060695	4.815216
289.899968	8000.099870	10.612391	-0.060692	4.815227
289.779772	8000.095786	10.617395	-0.060671	4.815226
289.924059	8000.081174	10.622400	-0.060699	4.815221
289.944431	8000.095502	10.627405	-0.060703	4.815225
289.706401	8000.081947	10.632410	-0.060660	4.815222
289.935861	8000.104072	10.637415	-0.060703	4.815228
289.898218	8000.091749	10.642419	-0.060697	4.815224
289.622421	8000.082907	10.647424	-0.060647	4.815223
289.786901	8000.084682	10.652429	-0.060678	4.815223
289.854596	8000.074131	10.657434	-0.060692	4.815219
290.014001	8000.111125	10.662439	-0.060722	4.815229
289.816173	8000.071501	10.667443	-0.060686	4.815219
289.789612	8000.059364	10.672448	-0.060682	4.815215
289.908330	8000.104231	10.677453	-0.060705	4.815228
289.739834	8000.074729	10.682458	-0.060675	4.815220
289.841136	8000.073302	10.687463	-0.060694	4.815219
289.896735	8000.037942	10.692467	-0.060706	4.815208
289.786602	8000.070400	10.697472	-0.060686	4.815218
290.011851	8000.082827	10.702477	-0.060729	4.815221
290.051100	8000.055750	10.707482	-0.060737	4.815213
290.144396	8000.103399	10.712487	-0.060755	4.815226
289.951197	8000.095947	10.717491	-0.060720	4.815225
290.121789	8000.103174	10.722496	-0.060753	4.815226
290.094872	8000.117777	10.727501	-0.060749	4.815231
289.871079	8000.078785	10.732506	-0.060708	4.815220
290.002607	8000.108891	10.737511	-0.060733	4.815228
289.932129	8000.106713	10.742515	-0.060721	4.815228
289.571906	8000.071845	10.747520	-0.060655	4.815220
289.733419	8000.075710	10.752525	-0.060685	4.815220
289.824972	8000.045235	10.757530	-0.060703	4.815211
290.085939	8000.077518	10.762535	-0.060753	4.815219
289.939639	8000.113647	10.767539	-0.060726	4.815230
289.947201	8000.112782	10.772544	-0.060729	4.815230
289.881217	8000.128867	10.777549	-0.060717	4.815235
289.866639	8000.068790	10.782554	-0.060715	4.815217
289.944730	8000.119393	10.787559	-0.060731	4.815232
289.983387	8000.096586	10.792563	-0.060739	4.815225
289.924319	8000.127763	10.797568	-0.060729	4.815234
290.001950	8000.137706	10.802573	-0.060744	4.815237
289.915731	8000.081773	10.807578	-0.060729	4.815221
290.191252	8000.102535	10.812583	-0.060781	4.815225
290.035458	8000.074315	10.817587	-0.060753	4.815218
289.931036	8000.069427	10.822592	-0.060734	4.815217
290.080480	8000.078438	10.827597	-0.060763	4.815219
289.995290	8000.065314	10.832602	-0.060748	4.815215
289.754809	8000.093440	10.837607	-0.060704	4.815225
289.969018	8000.101401	10.842611	-0.060745	4.815226
290.053322	8000.091130	10.847616	-0.060761	4.815222
290.105583	8000.126321	10.852621	-0.060772	4.815232
289.956922	8000.066128	10.857626	-0.060745	4.815216
289.984745	8000.152258	10.862631	-0.060751	4.815241
290.059857	8000.110808	10.867635	-0.060766	4.815228
290.021855	8000.111316	10.872640	-0.060760	4.815228
290.020491	8000.130627	10.877645	-0.060761	4.815234
289.986464	8000.095898	10.882650	-0.060755	4.815224
289.917392	8000.118349	10.887655	-0.060743	4.815231
290.062932	8000.127295	10.892659	-0.060771	4.815233
290.002330	8000.162727	10.897664	-0.060761	4.815243
290.163379	8000.171934	10.902669	-0.060791	4.815245
289.967631	8000.099180	10.907674	-0.060756	4.815225
290.253567	8000.130815	10.912679	-0.060810	4.815233
289.906286	8000.133607	10.917683	-0.060746	4.815235
290.064318	8000.106390	10.922688	-0.060776	4.815227
290.314792	8000.090357	10.927693	-0.060824	4.815221
289.958042	8000.073732	10.932698	-0.060758	4.815217
289.942517	8000.082107	10.937703	-0.060756	4.815220
290.054907	8000.086216	10.942707	-0.060778	4.815221
290.278660	8000.114665	10.947712	-0.060821	4.815228
290.224985	8000.132026	10.952717	-0.060811	4.815233
290.217640	8000.108445	10.957722	-0.060811	4.815226
290.282787	8000.107480	10.962727	-0.060824	4.815226
290.142291	8000.124449	10.967731	-0.060799	4.815231
290.123728	8000.110307	10.972736	-0.060796	4.815227
290.232439	8000.132541	10.977741	-0.060817	4.815233
290.028660	8000.101374	10.982746	-0.060780	4.815225
289.987117	8000.147824	10.987751	-0.060773	4.815239
290.020906	8000.123865	10.992755	-0.060780	4.815232
289.937221	8000.115046	10.997760	-0.060766	4.815229
290.024604	8000.175434	11.002765	-0.060783	4.815247
290.053179	8000.158876	11.007770	-0.060789	4.815242
290.097038	8000.161831	11.012775	-0.060798	4.815242
290.211517	8000.160627	11.017779	-0.060820	4.815241
290.115912	8000.099186	11.022784	-0.060803	4.815224
290.274985	8000.126547	11.027789	-0.060834	4.815231
290.117705	8000.073696	11.032794	-0.060805	4.815216
289.992531	8000.121948	11.037799	-0.060783	4.815231
290.318859	8000.102913	11.042803	-0.060844	4.815224
290.312855	8000.168149	11.047808	-0.060844	4.815243
290.263914	8000.180240	11.052813	-0.060836	4.815247
290.073918	8000.095814	11.057818	-0.060801	4.815223
290.104492	8000.137060	11.062823	-0.060808	4.815235
290.053639	8000.111676	11.067827	-0.060799	4.815227
289.883863	8000.066104	11.072832	-0.060769	4.815215
290.123225	8000.133329	11.077837	-0.060814	4.815233
290.257606	8000.104644	11.082842	-0.060840	4.815224
290.146402	8000.165969	11.087847	-0.060820	4.815243
290.088143	8000.145810	11.092851	-0.060810	4.815237
290.219372	8000.111723	11.097856	-0.060835	4.815227
290.329307	8000.098674	11.102861	-0.060857	4.815222
290.261010	8000.124347	11.107866	-0.060845	4.815230
290.251870	8000.142458	11.112871	-0.060844	4.815235
290.230855	8000.117576	11.117875	-0.060841	4.815228
290.156229	8000.124957	11.122880	-0.060828	4.815231
290.299453	8000.152051	11.127885	-0.060856	4.815238
290.227515	8000.110265	11.132890	-0.060843	4.815226
290.102196	8000.110373	11.137895	-0.060820	4.815227
290.120681	8000.132158	11.142899	-0.060825	4.815233
290.387973	8000.078965	11.147904	-0.060875	4.815216
290.213534	8000.100713	11.152909	-0.060844	4.815223
290.155241	8000.105158	11.157914	-0.060834	4.815225
290.245869	8000.129228	11.162919	-0.060852	4.815231
290.345457	8000.130982	11.167923	-0.060871	4.815231
290.138893	8000.101907	11.172928	-0.060833	4.815224
290.383442	8000.146755	11.177933	-0.060880	4.815236
290.357742	8000.128213	11.182938	-0.060876	4.815230
290.208766	8000.142900	11.187943	-0.060849	4.815235
290.243513	8000.107189	11.192947	-0.060856	4.815225
290.109114	8000.126401	11.197952	-0.060832	4.815231
290.094046	8000.131574	11.202957	-0.060830	4.815232
290.027074	8000.100570	11.207962	-0.060819	4.815224
290.141492	8000.138947	11.212967	-0.060841	4.815234
290.193353	8000.191249	11.217971	-0.060851	4.815249
290.227923	8000.145907	11.222976	-0.060859	4.815236
290.060925	8000.197734	11.227981	-0.060828	4.815252
290.287462	8000.156693	11.232986	-0.060871	4.815239
290.277655	8000.148047	11.237991	-0.060870	4.815236
290.106667	8000.112083	11.242995	-0.060839	4.815227
290.279875	8000.105448	11.248000	-0.060872	4.815224
290.338161	8000.148230	11.253005	-0.060884	4.815236
290.015108	8000.130032	11.258010	-0.060825	4.815232
290.234714	8000.130597	11.263015	-0.060867	4.815231
290.180328	8000.141527	11.268019	-0.060857	4.815235
290.134354	8000.106597	11.273024	-0.060850	4.815225
290.143679	8000.156043	11.278029	-0.060852	4.815239
290.147255	8000.141204	11.283034	-0.060854	4.815235
290.226308	8000.186475	11.288039	-0.060869	4.815247
290.226658	8000.210095	11.293043	-0.060870	4.815254
290.146442	8000.168169	11.298048	-0.060856	4.815242
290.469989	8000.180113	11.303053	-0.060917	4.815244
290.301632	8000.096050	11.308058	-0.060887	4.815221
290.157578	8000.119378	11.313063	-0.060861	4.815228
290.142528	8000.164135	11.318067	-0.060859	4.815241
290.127942	8000.121175	11.323072	-0.060857	4.815229
290.121163	8000.175699	11.328077	-0.060857	4.815245
290.120649	8000.161861	11.333082	-0.060858	4.815241
290.142147	8000.168719	11.338087	-0.060862	4.815242
289.922508	8000.147983	11.343091	-0.060822	4.815237
290.115255	8000.090326	11.348096	-0.060859	4.815220
290.064349	8000.087407	11.353101	-0.060850	4.815219
290.040935	8000.074253	11.358106	-0.060847	4.815215
290.242686	8000.131218	11.363111	-0.060885	4.815231
290.258859	8000.102682	11.368115	-0.060889	4.815222
290.189425	8000.079125	11.373120	-0.060877	4.815216
290.281714	8000.122480	11.378125	-0.060895	4.815228
290.322029	8000.097560	11.383130	-0.060904	4.815221
290.180479	8000.131629	11.388135	-0.060878	4.815231
290.096775	8000.165602	11.393139	-0.060863	4.815242
289.973300	8000.110111	11.398144	-0.060841	4.815226
290.247134	8000.126566	11.403149	-0.060893	4.815229
290.100340	8000.101707	11.408154	-0.060867	4.815223
290.026744	8000.151897	11.413159	-0.060854	4.815238
290.004460	8000.145181	11.418163	-0.060851	4.815236
290.082694	8000.095224	11.423168	-0.060866	4.815221
290.225506	8000.135150	11.428173	-0.060893	4.815232
290.161846	8000.093503	11.433178	-0.060882	4.815220
290.125947	8000.114373	11.438183	-0.060877	4.815226
290.341103	8000.106304	11.443187	-0.060917	4.815223
290.403360	8000.137385	11.448192	-0.060930	4.815232
290.510122	8000.140331	11.453197	-0.060951	4.815232
290.233085	8000.088672	11.458202	-0.060900	4.815218
290.316573	8000.116901	11.463207	-0.060916	4.815226
290.375488	8000.152205	11.468211	-0.060928	4.815236
290.181559	8000.098736	11.473216	-0.060893	4.815221
290.143403	8000.165571	11.478221	-0.060887	4.815241
290.181657	8000.093545	11.483226	-0.060895	4.815220
290.398811	8000.120814	11.488231	-0.060936	4.815227
290.100125	8000.079490	11.493235	-0.060881	4.815216
290.085682	8000.085744	11.498240	-0.060879	4.815218
290.385959	8000.129390	11.503245	-0.060936	4.815229
290.537726	8000.110627	11.508250	-0.060965	4.815223
290.242794	8000.134624	11.513255	-0.060911	4.815231
290.257642	8000.125324	11.518259	-0.060915	4.815228
290.210624	8000.104283	11.523264	-0.060907	4.815222
290.382829	8000.122238	11.528269	-0.060940	4.815227
290.370279	8000.066473	11.533274	-0.060938	4.815211
290.357718	8000.111272	11.538279	-0.060937	4.815224
290.270324	8000.114158	11.543283	-0.060922	4.815225
290.414981	8000.128440	11.548288	-0.060949	4.815228
290.339181	8000.119752	11.553293	-0.060936	4.815226
290.070561	8000.073585	11.558298	-0.060887	4.815214
290.242886	8000.087262	11.563303	-0.060920	4.815217
290.361978	8000.152465	11.568307	-0.060943	4.815236
290.192966	8000.098345	11.573312	-0.060912	4.815221
290.309230	8000.126056	11.578317	-0.060935	4.815228
290.255416	8000.115600	11.583322	-0.060926	4.815225
290.239790	8000.092948	11.588327	-0.060924	4.815219
290.256318	8000.202427	11.593331	-0.060928	4.815251
290.069193	8000.121257	11.598336	-0.060894	4.815228
290.251719	8000.199296	11.603341	-0.060928	4.815250
290.137803	8000.092613	11.608346	-0.060908	4.815219
290.129579	8000.110739	11.613351	-0.060907	4.815224
290.215189	8000.191425	11.618355	-0.060924	4.815247
290.288946	8000.125346	11.623360	-0.060939	4.815228
290.341970	8000.137015	11.628365	-0.060950	4.815231
290.416132	8000.090199	11.633370	-0.060964	4.815217
290.326964	8000.128359	11.638375	-0.060948	4.815228
290.271867	8000.162813	11.643379	-0.060939	4.815239
290.422059	8000.115138	11.648384	-0.060968	4.815224
290.628810	8000.173259	11.653389	-0.061007	4.815240
290.381158	8000.124234	11.658394	-0.060962	4.815227
290.224466	8000.135581	11.663399	-0.060934	4.815231
290.495964	8000.183024	11.668403	-0.060985	4.815243
290.587726	8000.130085	11.673408	-0.061003	4.815227
290.527083	8000.162307	11.678413	-0.060993	4.815237
290.437660	8000.108457	11.683418	-0.060977	4.815222
290.396942	8000.114268	11.688423	-0.060970	4.815224
290.424959	8000.114818	11.693427	-0.060976	4.815224
290.396762	8000.128329	11.698432	-0.060972	4.815228
290.310158	8000.107691	11.703437	-0.060956	4.815222
290.456761	8000.134844	11.708442	-0.060985	4.815229
290.244382	8000.113159	11.713447	-0.060946	4.815224
290.197237	8000.113513	11.718451	-0.060938	4.815224
290.338425	8000.086012	11.723456	-0.060965	4.815216
290.491903	8000.147515	11.728461	-0.060995	4.815233
290.236636	8000.058778	11.733466	-0.060948	4.815208
290.530589	8000.083062	11.738471	-0.061004	4.815214
290.456413	8000.074402	11.743475	-0.060991	4.815212
290.149029	8000.055397	11.748480	-0.060934	4.815207
290.511093	8000.148227	11.753485	-0.061003	4.815233
290.390512	8000.082085	11.758490	-0.060981	4.815214
290.331885	8000.084385	11.763495	-0.060971	4.815215
290.398236	8000.090929	11.768499	-0.060984	4.815217
290.595538	8000.079351	11.773504	-0.061022	4.815212
290.351988	8000.108493	11.778509	-0.060977	4.815222
290.354662	8000.119315	11.783514	-0.060979	4.815225
290.542948	8000.123633	11.788519	-0.061014	4.815225
290.710396	8000.108343	11.793523	-0.061046	4.815220
290.544247	8000.112042	11.798528	-0.061016	4.815222
290.335659	8000.115027	11.803533	-0.060978	4.815224
290.381659	8000.090203	11.808538	-0.060988	4.815216
290.384026	8000.121346	11.813543	-0.060989	4.815225
290.366376	8000.115777	11.818547	-0.060987	4.815224
290.385535	8000.079804	11.823552	-0.060991	4.815213
290.527393	8000.137901	11.828557	-0.061018	4.815229
290.507658	8000.084155	11.833562	-0.061016	4.815214
290.687684	8000.112941	11.838567	-0.061050	4.815221
290.609668	8000.213340	11.843571	-0.061036	4.815251
290.325465	8000.135883	11.848576	-0.060984	4.815230
290.522721	8000.174587	11.853581	-0.061022	4.815240
290.533008	8000.158790	11.858586	-0.061025	4.815235
290.357518	8000.129167	11.863591	-0.060993	4.815227
290.296605	8000.103613	11.868595	-0.060982	4.815220
290.370860	8000.082475	11.873600	-0.060997	4.815214
290.514008	8000.138455	11.878605	-0.061025	4.815229
290.430417	8000.080424	11.883610	-0.061010	4.815213
290.559835	8000.092309	11.888615	-0.061035	4.815216
290.531765	8000.129359	11.893619	-0.061030	4.815227
290.337911	8000.091938	11.898624	-0.060995	4.815217
290.397215	8000.120830	11.903629	-0.061007	4.815225
290.466893	8000.075008	11.908634	-0.061021	4.815211
290.552140	8000.117175	11.913639	-0.061038	4.815223
290.578320	8000.148719	11.918643	-0.061043	4.815232
290.335429	8000.101914	11.923648	-0.060999	4.815219
290.400324	8000.127690	11.928653	-0.061012	4.815227
290.385050	8000.109324	11.933658	-0.061010	4.815221
290.470693	8000.098006	11.938663	-0.061027	4.815217
290.540143	8000.147396	11.943667	-0.061041	4.815232
290.458295	8000.107581	11.948672	-0.061026	4.815220
290.370942	8000.128655	11.953677	-0.061011	4.815227
290.559224	8000.141532	11.958682	-0.061047	4.815230
290.478641	8000.129554	11.963687	-0.061033	4.815227
290.405895	8000.131616	11.968691	-0.061020	4.815227
290.532682	8000.124201	11.973696	-0.061044	4.815225
290.548054	8000.144865	11.978701	-0.061048	4.815231
290.495980	8000.131227	11.983706	-0.061039	4.815227
290.415989	8000.137447	11.988711	-0.061025	4.815229
290.558161	8000.180573	11.993715	-0.061053	4.815241
290.442321	8000.099532	11.998720	-0.061032	4.815218
290.599002	8000.158950	12.003725	-0.061062	4.815234
290.485205	8000.122877	12.008730	-0.061042	4.815224
290.535367	8000.129148	12.013735	-0.061052	4.815226
290.337168	8000.120539	12.018739	-0.061016	4.815224
290.602270	8000.101545	12.023744	-0.061066	4.815217
290.645489	8000.130167	12.028749	-0.061075	4.815226
290.392693	8000.091752	12.033754	-0.061029	4.815216
290.535632	8000.102796	12.038759	-0.061056	4.815218
290.641634	8000.135684	12.043763	-0.061077	4.815227
290.499196	8000.108757	12.048768	-0.061051	4.815220
290.460064	8000.147760	12.053773	-0.061045	4.815232
290.532807	8000.109479	12.058778	-0.061059	4.815220
290.731160	8000.111827	12.063783	-0.061097	4.815220
290.675236	8000.158037	12.068787	-0.061087	4.815233
290.782188	8000.136379	12.073792	-0.061108	4.815227
290.729119	8000.145192	12.078797	-0.061099	4.815229
290.570485	8000.150087	12.083802	-0.061070	4.815232
290.363147	8000.132765	12.088807	-0.061033	4.815227
290.688827	8000.141537	12.093811	-0.061094	4.815228
290.715483	8000.104619	12.098816	-0.061100	4.815217
290.496083	8000.142726	12.103821	-0.061060	4.815230
290.593956	8000.117706	12.108826	-0.061079	4.815222
290.658077	8000.125283	12.113831	-0.061092	4.815224
290.679145	8000.195256	12.118835	-0.061097	4.815244
290.556408	8000.108749	12.123840	-0.061075	4.815219
290.752474	8000.158132	12.128845	-0.061112	4.815233
290.581052	8000.111459	12.133850	-0.061081	4.815220
290.477060	8000.103367	12.138855	-0.061062	4.815218
290.706247	8000.113724	12.143859	-0.061106	4.815220
290.473191	8000.086340	12.148864	-0.061063	4.815213
290.451046	8000.114931	12.153869	-0.061060	4.815222
290.649885	8000.120497	12.158874	-0.061098	4.815222
290.650441	8000.130213	12.163879	-0.061099	4.815225
290.616122	8000.126503	12.168883	-0.061094	4.815224
290.603183	8000.107106	12.173888	-0.061092	4.815218
290.737308	8000.151167	12.178893	-0.061118	4.815231
290.628002	8000.179359	12.183898	-0.061098	4.815239
290.719428	8000.185257	12.188903	-0.061116	4.815241
290.614407	8000.186775	12.193907	-0.061098	4.815242
290.867732	8000.134418	12.198912	-0.061146	4.815225
290.525117	8000.128725	12.203917	-0.061083	4.815225
290.384948	8000.082579	12.208922	-0.061057	4.815212
290.589427	8000.108567	12.213927	-0.061096	4.815219
290.618126	8000.116617	12.218931	-0.061102	4.815221
290.528161	8000.098062	12.223936	-0.061087	4.815216
290.691474	8000.126567	12.228941	-0.061118	4.815223
290.712725	8000.159098	12.233946	-0.061123	4.815233
290.403605	8000.104757	12.238951	-0.061066	4.815218
290.680612	8000.127687	12.243955	-0.061118	4.815224
290.498730	8000.082978	12.248960	-0.061085	4.815212
290.486955	8000.127791	12.253965	-0.061084	4.815225
290.529149	8000.120021	12.258970	-0.061093	4.815222
290.541093	8000.102112	12.263975	-0.061096	4.815217
290.795387	8000.079727	12.268979	-0.061144	4.815209
290.755806	8000.082348	12.273984	-0.061138	4.815210
290.789785	8000.116163	12.278989	-0.061145	4.815220
290.747307	8000.078081	12.283994	-0.061138	4.815209
290.561398	8000.091075	12.288999	-0.061104	4.815213
290.753067	8000.131826	12.294003	-0.061141	4.815224
290.849234	8000.092869	12.299008	-0.061159	4.815212
290.740669	8000.148891	12.304013	-0.061140	4.815229
290.608931	8000.111445	12.309018	-0.061116	4.815219
290.589297	8000.111192	12.314023	-0.061113	4.815219
290.621476	8000.165304	12.319027	-0.061120	4.815235
290.387144	8000.128270	12.324032	-0.061078	4.815225
290.562983	8000.163405	12.329037	-0.061111	4.815234
290.801256	8000.182474	12.334042	-0.061156	4.815239
290.714551	8000.130808	12.339047	-0.061141	4.815224
290.629937	8000.132671	12.344051	-0.061126	4.815225
290.707362	8000.089119	12.349056	-0.061141	4.815212
290.584542	8000.116014	12.354061	-0.061119	4.815220
290.435971	8000.127498	12.359066	-0.061093	4.815224
290.622618	8000.128580	12.364071	-0.061128	4.815224
290.691850	8000.165129	12.369075	-0.061142	4.815234
290.449648	8000.101216	12.374080	-0.061098	4.815217
290.625764	8000.124587	12.379085	-0.061131	4.815222
290.727971	8000.141364	12.384090	-0.061151	4.815227
290.672836	8000.111627	12.389095	-0.061142	4.815218
290.698972	8000.133542	12.394099	-0.061148	4.815225
290.662601	8000.124449	12.399104	-0.061142	4.815222
290.546391	8000.119360	12.404109	-0.061121	4.815221
290.475111	8000.136425	12.409114	-0.061109	4.815227
290.577232	8000.102917	12.414119	-0.061128	4.815216
290.861642	8000.136672	12.419123	-0.061182	4.815225
290.539764	8000.089604	12.424128	-0.061123	4.815212
290.602956	8000.130331	12.429133	-0.061136	4.815224
290.602940	8000.086544	12.434138	-0.061137	4.815211
290.612739	8000.075019	12.439143	-0.061139	4.815208
290.683825	8000.121228	12.444147	-0.061153	4.815221
290.668913	8000.081470	12.449152	-0.061152	4.815209
290.777437	8000.142218	12.454157	-0.061173	4.815227
290.628226	8000.119455	12.459162	-0.061146	4.815221
290.742184	8000.109684	12.464167	-0.061168	4.815217
290.834770	8000.120950	12.469171	-0.061186	4.815220
290.494071	8000.106731	12.474176	-0.061123	4.815217
290.678364	8000.121681	12.479181	-0.061158	4.815221
290.741579	8000.148500	12.484186	-0.061171	4.815228
290.681007	8000.122951	12.489191	-0.061161	4.815221
290.854495	8000.140929	12.494195	-0.061194	4.815226
290.766431	8000.125616	12.499200	-0.061178	4.815222
290.882934	8000.152263	12.504205	-0.061201	4.815229
290.913362	8000.107919	12.509210	-0.061207	4.815216
290.763537	8000.125801	12.514215	-0.061180	4.815222
290.846714	8000.137978	12.519219	-0.061197	4.815225
290.638272	8000.114218	12.524224	-0.061159	4.815219
290.809208	8000.135362	12.529229	-0.061191	4.815224
290.755507	8000.115278	12.534234	-0.061182	4.815218
290.684149	8000.117364	12.539239	-0.061170	4.815219
290.712728	8000.122202	12.544243	-0.061176	4.815221
290.789419	8000.093616	12.549248	-0.061191	4.815212
290.701490	8000.129658	12.554253	-0.061176	4.815223
290.658948	8000.102273	12.559258	-0.061169	4.815215
290.803332	8000.104783	12.564263	-0.061196	4.815215
290.911714	8000.116315	12.569267	-0.061217	4.815218
290.817116	8000.111590	12.574272	-0.061201	4.815217
290.699240	8000.155686	12.579277	-0.061180	4.815230
290.760359	8000.107580	12.584282	-0.061192	4.815216
290.761342	8000.092696	12.589287	-0.061193	4.815212
290.841334	8000.101611	12.594291	-0.061209	4.815214
290.774119	8000.117674	12.599296	-0.061197	4.815219
290.811549	8000.138710	12.604301	-0.061205	4.815225
290.838870	8000.106082	12.609306	-0.061211	4.815215
290.558099	8000.103570	12.614311	-0.061159	4.815216
290.797053	8000.137629	12.619315	-0.061205	4.815224
290.826785	8000.090064	12.624320	-0.061211	4.815210
290.739050	8000.115411	12.629325	-0.061196	4.815218
290.712840	8000.115047	12.634330	-0.061192	4.815218
290.676231	8000.129487	12.639335	-0.061186	4.815222
290.892214	8000.132133	12.644339	-0.061227	4.815222
290.752879	8000.109536	12.649344	-0.061202	4.815216
290.675275	8000.129704	12.654349	-0.061188	4.815222
290.687519	8000.116080	12.659354	-0.061191	4.815218
290.647410	8000.097295	12.664359	-0.061185	4.815213
290.640391	8000.107953	12.669363	-0.061184	4.815216
290.505446	8000.088640	12.674368	-0.061160	4.815211
290.500336	8000.137845	12.679373	-0.061160	4.815226
290.759653	8000.095217	12.684378	-0.061209	4.815212
290.633461	8000.119916	12.689383	-0.061186	4.815220
290.566482	8000.128495	12.694387	-0.061175	4.815222
290.480734	8000.117499	12.699392	-0.061160	4.815220
290.657213	8000.141947	12.704397	-0.061193	4.815226
290.677933	8000.146654	12.709402	-0.061198	4.815227
290.473136	8000.136862	12.714407	-0.061161	4.815225
290.589467	8000.145319	12.719411	-0.061183	4.815227
290.546420	8000.135043	12.724416	-0.061176	4.815224
290.666362	8000.144630	12.729421	-0.061199	4.815227
290.733349	8000.156535	12.734426	-0.061213	4.815230
290.673526	8000.119230	12.739431	-0.061202	4.815219
290.896870	8000.144468	12.744435	-0.061245	4.815225
290.641532	8000.113498	12.749440	-0.061198	4.815217
290.856644	8000.110780	12.754445	-0.061239	4.815216
290.935240	8000.159256	12.759450	-0.061255	4.815229
290.759956	8000.123215	12.764455	-0.061223	4.815220
290.984322	8000.133492	12.769459	-0.061265	4.815222
291.056687	8000.105903	12.774464	-0.061280	4.815213
290.930604	8000.122044	12.779469	-0.061257	4.815218
290.921209	8000.115545	12.784474	-0.061256	4.815217
290.812412	8000.103091	12.789479	-0.061237	4.815213
290.869991	8000.153353	12.794483	-0.061248	4.815228
290.923977	8000.084799	12.799488	-0.061259	4.815207
290.966553	8000.110201	12.804493	-0.061268	4.815215
291.003837	8000.120536	12.809498	-0.061276	4.815217
290.680020	8000.095901	12.814503	-0.061216	4.815212
290.859949	8000.122547	12.819507	-0.061251	4.815219
290.841258	8000.107332	12.824512	-0.061248	4.815214
290.924921	8000.137706	12.829517	-0.061265	4.815223
290.889521	8000.106161	12.834522	-0.061259	4.815214
290.964550	8000.118202	12.839527	-0.061274	4.815217
291.141253	8000.175821	12.844531	-0.061308	4.815233
290.794417	8000.111212	12.849536	-0.061244	4.815216
290.846173	8000.133559	12.854541	-0.061254	4.815222
290.844847	8000.187108	12.859546	-0.061255	4.815237
290.643148	8000.137783	12.864551	-0.061218	4.815224
290.812419	8000.148202	12.869555	-0.061251	4.815226
290.903908	8000.128424	12.874560	-0.061268	4.815220
290.844372	8000.158525	12.879565	-0.061258	4.815229
290.832515	8000.181941	12.884570	-0.061257	4.815236
290.954650	8000.141281	12.889575	-0.061281	4.815223
291.009362	8000.164748	12.894579	-0.061292	4.815230
290.830811	8000.148979	12.899584	-0.061259	4.815226
291.113517	8000.160240	12.904589	-0.061313	4.815228
291.115402	8000.194586	12.909594	-0.061314	4.815238
290.817490	8000.141500	12.914599	-0.061259	4.815224
290.987345	8000.164767	12.919603	-0.061292	4.815230
291.006748	8000.134145	12.924608	-0.061296	4.815221
291.077810	8000.134351	12.929613	-0.061310	4.815221
290.886258	8000.142970	12.934618	-0.061276	4.815224
290.859898	8000.117997	12.939623	-0.061271	4.815217
291.018735	8000.182804	12.944627	-0.061302	4.815235
290.956198	8000.134753	12.949632	-0.061291	4.815221
291.011760	8000.125068	12.954637	-0.061302	4.815218
290.932622	8000.127023	12.959642	-0.061288	4.815219
290.727129	8000.143966	12.964647	-0.061251	4.815225
290.876857	8000.139077	12.969651	-0.061280	4.815223
290.783538	8000.135443	12.974656	-0.061263	4.815222
290.764432	8000.111662	12.979661	-0.061261	4.815215
290.762518	8000.138454	12.984666	-0.061261	4.815223
290.762973	8000.124632	12.989671	-0.061262	4.815219
290.944002	8000.128829	12.994675	-0.061297	4.815219
290.648426	8000.074714	12.999680	-0.061242	4.815205
290.802544	8000.125532	13.004685	-0.061272	4.815219
290.721317	8000.110333	13.009690	-0.061258	4.815215
290.990974	8000.114954	13.014695	-0.061309	4.815215
291.011754	8000.147479	13.019699	-0.061314	4.815224
291.039768	8000.096674	13.024704	-0.061320	4.815209
291.043939	8000.136408	13.029709	-0.061321	4.815221
290.835362	8000.121203	13.034714	-0.061283	4.815217
290.952598	8000.117907	13.039719	-0.061306	4.815216
290.995518	8000.142245	13.044723	-0.061315	4.815223
290.764113	8000.114887	13.049728	-0.061273	4.815216
290.775619	8000.117298	13.054733	-0.061276	4.815217
290.869350	8000.130724	13.059738	-0.061294	4.815220
291.071748	8000.122444	13.064743	-0.061332	4.815217
290.882377	8000.173895	13.069747	-0.061298	4.815232
290.937037	8000.137448	13.074752	-0.061309	4.815222
290.858995	8000.170447	13.079757	-0.061295	4.815232
290.979087	8000.152220	13.084762	-0.061319	4.815226
291.040775	8000.121241	13.089767	-0.061331	4.815216
291.227804	8000.192944	13.094771	-0.061367	4.815236
291.027041	8000.160751	13.099776	-0.061330	4.815228
290.841824	8000.155569	13.104781	-0.061297	4.815227
291.014126	8000.168179	13.109786	-0.061330	4.815230
291.004514	8000.156326	13.114791	-0.061329	4.815227
290.940993	8000.164963	13.119795	-0.061318	4.815229
290.967383	8000.136598	13.124800	-0.061323	4.815221
291.008080	8000.144851	13.129805	-0.061332	4.815223
290.987914	8000.146729	13.134810	-0.061329	4.815224
290.825197	8000.128017	13.139815	-0.061299	4.815219
291.085236	8000.156014	13.144819	-0.061349	4.815226
290.891344	8000.151755	13.149824	-0.061314	4.815226
291.028322	8000.166980	13.154829	-0.061340	4.815229
290.913832	8000.149080	13.159834	-0.061319	4.815225
290.809919	8000.133498	13.164839	-0.061301	4.815221
290.838644	8000.134060	13.169843	-0.061307	4.815221
290.986048	8000.134482	13.174848	-0.061335	4.815220
291.063881	8000.169038	13.179853	-0.061351	4.815230
290.933506	8000.146591	13.184858	-0.061327	4.815224
290.933264	8000.129547	13.189863	-0.061328	4.815219
291.194430	8000.165053	13.194867	-0.061378	4.815228
290.788771	8000.125128	13.199872	-0.061303	4.815218
290.673870	8000.112572	13.204877	-0.061282	4.815215
290.855603	8000.140319	13.209882	-0.061317	4.815222
291.016944	8000.125997	13.214887	-0.061348	4.815217
290.842617	8000.153094	13.219891	-0.061316	4.815226
290.902636	8000.142415	13.224896	-0.061329	4.815222
291.068408	8000.187012	13.229901	-0.061360	4.815235
291.130305	8000.171015	13.234906	-0.061373	4.815230
290.881195	8000.172244	13.239911	-0.061327	4.815231
291.004909	8000.174407	13.244915	-0.061351	4.815231
290.889485	8000.139373	13.249920	-0.061330	4.815222
290.760434	8000.172583	13.254925	-0.061307	4.815232
290.921651	8000.163608	13.259930	-0.061338	4.815228
291.020093	8000.118270	13.264935	-0.061357	4.815215
291.034489	8000.171015	13.269939	-0.061361	4.815230
291.036586	8000.144381	13.274944	-0.061362	4.815222
290.919141	8000.155319	13.279949	-0.061341	4.815226
290.914738	8000.189559	13.284954	-0.061341	4.815236
290.765797	8000.119724	13.289959	-0.061314	4.815216
290.817399	8000.133510	13.294963	-0.061325	4.815220
290.999499	8000.123818	13.299968	-0.061359	4.815216
290.659590	8000.131007	13.304973	-0.061297	4.815220
290.759192	8000.143462	13.309978	-0.061316	4.815223
290.817995	8000.143461	13.314983	-0.061328	4.815223
290.791254	8000.182674	13.319987	-0.061324	4.815234
290.785732	8000.139863	13.324992	-0.061324	4.815222
290.946178	8000.171532	13.329997	-0.061355	4.815230
291.118357	8000.196979	13.335002	-0.061388	4.815237
290.931216	8000.179995	13.340007	-0.061354	4.815233
291.143169	8000.196483	13.345011	-0.061394	4.815237
291.046610	8000.220611	13.350016	-0.061377	4.815244
290.912077	8000.180976	13.355021	-0.061353	4.815233
291.265462	8000.185940	13.360026	-0.061419	4.815233
291.112172	8000.138499	13.365031	-0.061392	4.815220
290.987039	8000.130048	13.370035	-0.061369	4.815218
290.904181	8000.101983	13.375040	-0.061355	4.815210
290.963141	8000.154409	13.380045	-0.061366	4.815225
291.082372	8000.157566	13.385050	-0.061390	4.815225
290.930975	8000.160442	13.390055	-0.061362	4.815227
291.131349	8000.199203	13.395059	-0.061400	4.815237
291.010326	8000.191892	13.400064	-0.061379	4.815236
290.979629	8000.156146	13.405069	-0.061374	4.815225
291.005574	8000.180199	13.410074	-0.061380	4.815232
290.987481	8000.158574	13.415079	-0.061377	4.815226
291.065351	8000.219878	13.420083	-0.061392	4.815243
290.942004	8000.157964	13.425088	-0.061370	4.815226
291.066669	8000.158003	13.430093	-0.061394	4.815225
291.120161	8000.125816	13.435098	-0.061405	4.815216
290.888460	8000.145526	13.440103	-0.061363	4.815222
291.126838	8000.164600	13.445107	-0.061408	4.815227
290.926528	8000.152743	13.450112	-0.061372	4.815224
290.929176	8000.163564	13.455117	-0.061373	4.815227
290.895220	8000.153441	13.460122	-0.061368	4.815225
290.869313	8000.133824	13.465127	-0.061364	4.815219
290.972254	8000.180572	13.470131	-0.061384	4.815232
290.863637	8000.206637	13.475136	-0.061364	4.815240
290.883859	8000.158911	13.480141	-0.061369	4.815226
290.992125	8000.173652	13.485146	-0.061390	4.815230
290.832072	8000.134656	13.490151	-0.061361	4.815219
290.979678	8000.167179	13.495155	-0.061389	4.815228
290.941193	8000.163398	13.500160	-0.061383	4.815227
291.036570	8000.177922	13.505165	-0.061402	4.815231
290.948899	8000.185082	13.510170	-0.061386	4.815233
291.007062	8000.135855	13.515175	-0.061398	4.815219
291.060150	8000.181763	13.520179	-0.061409	4.815232
290.946945	8000.126439	13.525184	-0.061388	4.815216
291.001496	8000.135995	13.530189	-0.061399	4.815219
291.243122	8000.155124	13.535194	-0.061445	4.815223
290.915249	8000.151816	13.540199	-0.061385	4.815224
290.837518	8000.185890	13.545203	-0.061372	4.815234
291.037574	8000.165802	13.550208	-0.061410	4.815227
291.071508	8000.145054	13.555213	-0.061417	4.815221
291.001501	8000.142882	13.560218	-0.061405	4.815221
290.995807	8000.126816	13.565223	-0.061404	4.815216
291.081989	8000.171142	13.570227	-0.061421	4.815228
290.817501	8000.112198	13.575232	-0.061373	4.815212
290.964190	8000.129726	13.580237	-0.061401	4.815217
291.267682	8000.145618	13.585242	-0.061458	4.815220
291.137471	8000.121034	13.590247	-0.061435	4.815213
291.083392	8000.111641	13.595251	-0.061426	4.815211
291.031551	8000.121544	13.600256	-0.061417	4.815214
291.103100	8000.147436	13.605261	-0.061431	4.815221
291.098888	8000.142093	13.610266	-0.061431	4.815220
291.086877	8000.126990	13.615271	-0.061430	4.815215
291.205232	8000.148321	13.620275	-0.061453	4.815221
290.930973	8000.126658	13.625280	-0.061403	4.815216
290.849776	8000.117878	13.630285	-0.061388	4.815214
291.005533	8000.186915	13.635290	-0.061418	4.815233
290.939448	8000.127035	13.640295	-0.061407	4.815216
290.998157	8000.168758	13.645299	-0.061419	4.815228
291.140052	8000.178717	13.650304	-0.061446	4.815230
291.045159	8000.138679	13.655309	-0.061429	4.815219
291.177529	8000.130289	13.660314	-0.061455	4.815216
291.247163	8000.097304	13.665319	-0.061468	4.815206
291.292440	8000.144151	13.670323	-0.061478	4.815219
291.341101	8000.115092	13.675328	-0.061488	4.815210
291.233677	8000.159365	13.680333	-0.061469	4.815224
291.302319	8000.177718	13.685338	-0.061482	4.815229
291.052864	8000.135075	13.690343	-0.061437	4.815217
291.007643	8000.177186	13.695347	-0.061429	4.815230
291.275455	8000.177499	13.700352	-0.061480	4.815229
291.236225	8000.139469	13.705357	-0.061473	4.815218
291.134131	8000.158154	13.710362	-0.061455	4.815224
290.998621	8000.135620	13.715367	-0.061431	4.815218
291.089971	8000.155426	13.720371	-0.061449	4.815223
291.144290	8000.126462	13.725376	-0.061460	4.815214
291.151886	8000.153416	13.730381	-0.061462	4.815222
291.399436	8000.216512	13.735386	-0.061509	4.815239
291.434778	8000.175459	13.740391	-0.061516	4.815227
291.256672	8000.159695	13.745395	-0.061484	4.815223
291.325597	8000.186613	13.750400	-0.061498	4.815231
291.077636	8000.158973	13.755405	-0.061452	4.815224
291.142737	8000.170848	13.760410	-0.061465	4.815227
291.123713	8000.131019	13.765415	-0.061463	4.815216
291.361623	8000.201441	13.770419	-0.061508	4.815235
291.257062	8000.221154	13.775424	-0.061489	4.815241
291.086078	8000.161645	13.780429	-0.061458	4.815225
290.993557	8000.184771	13.785434	-0.061442	4.815232
291.007997	8000.134807	13.790439	-0.061445	4.815217
291.081275	8000.175707	13.795443	-0.061460	4.815229
291.145673	8000.156542	13.800448	-0.061473	4.815223
291.069539	8000.153197	13.805453	-0.061459	4.815222
291.115397	8000.161537	13.810458	-0.061469	4.815224
290.904594	8000.146293	13.815463	-0.061430	4.815221
291.125667	8000.184334	13.820467	-0.061473	4.815231
291.180214	8000.157514	13.825472	-0.061484	4.815223
290.858572	8000.170359	13.830477	-0.061425	4.815228
291.047146	8000.204642	13.835482	-0.061461	4.815237
291.095713	8000.157393	13.840487	-0.061470	4.815223
290.971180	8000.187469	13.845491	-0.061448	4.815232
291.005410	8000.202033	13.850496	-0.061455	4.815237
290.986906	8000.185750	13.855501	-0.061453	4.815232
291.074379	8000.190512	13.860506	-0.061470	4.815233
291.179262	8000.146352	13.865511	-0.061490	4.815219
291.206557	8000.166149	13.870515	-0.061496	4.815225
291.181096	8000.161518	13.875520	-0.061492	4.815224
290.864892	8000.155196	13.880525	-0.061434	4.815223
290.999923	8000.202486	13.885530	-0.061460	4.815237
291.066005	8000.158742	13.890535	-0.061473	4.815223
291.150641	8000.150617	13.895539	-0.061490	4.815221
291.097692	8000.170131	13.900544	-0.061481	4.815227
291.402060	8000.152872	13.905549	-0.061539	4.815220
291.313865	8000.152533	13.910554	-0.061523	4.815220
291.025377	8000.116720	13.915559	-0.061470	4.815211
291.071268	8000.175347	13.920563	-0.061480	4.815228
291.185211	8000.154877	13.925568	-0.061502	4.815222
291.025076	8000.124438	13.930573	-0.061473	4.815213
291.199219	8000.134941	13.935578	-0.061506	4.815216
291.218016	8000.120357	13.940583	-0.061510	4.815211
291.175515	8000.163585	13.945587	-0.061503	4.815224
291.166861	8000.117511	13.950592	-0.061503	4.815211
291.133605	8000.161964	13.955597	-0.061497	4.815224
291.331146	8000.209239	13.960602	-0.061535	4.815237
291.099927	8000.173321	13.965607	-0.061493	4.815227
291.308722	8000.194038	13.970611	-0.061532	4.815232
291.255394	8000.209265	13.975616	-0.061523	4.815237
291.096423	8000.190615	13.980621	-0.061495	4.815232
291.320756	8000.225502	13.985626	-0.061537	4.815241
291.049621	8000.164304	13.990631	-0.061488	4.815225
291.016574	8000.163825	13.995635	-0.061482	4.815225
291.041033	8000.193202	14.000640	-0.061488	4.815233
291.088781	8000.178037	14.005645	-0.061498	4.815228
291.237071	8000.216991	14.010650	-0.061526	4.815239
291.149419	8000.151397	14.015655	-0.061511	4.815220
291.360242	8000.153959	14.020659	-0.061551	4.815220
291.177244	8000.106016	14.025664	-0.061517	4.815207
291.065457	8000.139517	14.030669	-0.061497	4.815217
291.206263	8000.153737	14.035674	-0.061525	4.815221
291.208103	8000.155986	14.040679	-0.061526	4.815221
291.245394	8000.156693	14.045683	-0.061534	4.815221
291.039729	8000.200379	14.050688	-0.061496	4.815235
290.999875	8000.168758	14.055693	-0.061490	4.815226
291.307277	8000.197556	14.060698	-0.061548	4.815233
291.175427	8000.109819	14.065703	-0.061524	4.815208
291.293689	8000.165386	14.070707	-0.061547	4.815223
291.310367	8000.187143	14.075712	-0.061551	4.815230
291.218157	8000.143940	14.080717	-0.061534	4.815217
291.325697	8000.193977	14.085722	-0.061555	4.815232
291.468576	8000.162227	14.090727	-0.061583	4.815222
291.119798	8000.181032	14.095731	-0.061519	4.815229
291.200142	8000.201723	14.100736	-0.061535	4.815234
291.258615	8000.153571	14.105741	-0.061546	4.815220
291.477057	8000.209758	14.110746	-0.061588	4.815235
291.325795	8000.159139	14.115751	-0.061561	4.815221
291.267034	8000.162506	14.120755	-0.061550	4.815222
291.286991	8000.138313	14.125760	-0.061555	4.815215
291.256144	8000.160339	14.130765	-0.061550	4.815222
291.271640	8000.190635	14.135770	-0.061554	4.815231
291.307124	8000.138886	14.140775	-0.061561	4.815215
291.331642	8000.143657	14.145779	-0.061567	4.815217
291.452419	8000.154330	14.150784	-0.061590	4.815219
291.171277	8000.130410	14.155789	-0.061539	4.815213
291.342969	8000.182599	14.160794	-0.061572	4.815228
291.284025	8000.200941	14.165799	-0.061561	4.815233
291.264634	8000.176084	14.170803	-0.061559	4.815226
291.328399	8000.165468	14.175808	-0.061571	4.815223
291.327290	8000.164458	14.180813	-0.061572	4.815222
291.225315	8000.208823	14.185818	-0.061554	4.815236
291.383469	7999.241179	14.190823	-0.061584	4.814953
291.041495	7996.050870	14.195827	-0.061519	4.814023
291.256987	7990.609891	14.200832	-0.061556	4.812434
291.204770	7983.878222	14.205837	-0.061543	4.810468
291.143488	7976.652373	14.210842	-0.061528	4.808358
291.011320	7968.960845	14.215847	-0.061499	4.806110
291.031121	7961.218818	14.220851	-0.061498	4.803846
291.286509	7953.361455	14.225856	-0.061542	4.801546
291.019238	7945.339696	14.230861	-0.061488	4.799199
291.022806	7937.475340	14.235866	-0.061484	4.796896
291.072834	7929.390690	14.240871	-0.061489	4.794527
291.053342	7921.393101	14.245875	-0.061481	4.792183
290.935693	7913.347972	14.250880	-0.061455	4.789824
290.805851	7905.396034	14.255885	-0.061426	4.787491
290.982614	7897.374819	14.260890	-0.061455	4.785135
290.900532	7889.445215	14.265895	-0.061435	4.782807
290.820128	7881.387827	14.270899	-0.061416	4.780439
290.882378	7873.434105	14.275904	-0.061423	4.778101
290.653910	7865.366769	14.280909	-0.061376	4.775729
290.726456	7857.375447	14.285914	-0.061385	4.773376
290.664689	7849.307825	14.290919	-0.061369	4.771001
290.734522	7841.336023	14.295923	-0.061378	4.768653
290.572334	7833.358800	14.300928	-0.061343	4.766302
290.461654	7825.366121	14.305933	-0.061318	4.763945
290.639589	7817.466728	14.310938	-0.061347	4.761614
290.472819	7809.354380	14.315943	-0.061312	4.759220
290.525067	7801.398901	14.320947	-0.061317	4.756871
290.522347	7793.354785	14.325952	-0.061312	4.754494
290.395601	7785.274187	14.330957	-0.061284	4.752106
290.414638	7777.331292	14.335962	-0.061284	4.749756
290.306787	7769.286473	14.340967	-0.061259	4.747376
290.397305	7761.295374	14.345971	-0.061272	4.745010
290.442830	7753.344625	14.350976	-0.061276	4.742655
290.054385	7745.295230	14.355981	-0.061199	4.740270
290.220364	7737.361123	14.360986	-0.061226	4.737917
290.178157	7729.288823	14.365991	-0.061213	4.735523
289.983977	7721.312687	14.370995	-0.061173	4.733156
290.015633	7713.245109	14.376000	-0.061174	4.730760
289.847195	7705.264763	14.381005	-0.061139	4.728390
289.855751	7697.330076	14.386010	-0.061136	4.726031
289.894023	7689.288386	14.391015	-0.061139	4.723639
289.935127	7681.335751	14.396019	-0.061142	4.721273
289.862323	7673.352527	14.401024	-0.061124	4.718896
289.732834	7665.337235	14.406029	-0.061096	4.716509
289.816697	7657.323693	14.411034	-0.061107	4.714121
289.796455	7649.255741	14.416039	-0.061099	4.711715
289.727826	7641.270001	14.421043	-0.061082	4.709333
289.855448	7633.306631	14.426048	-0.061101	4.706956
289.722236	7625.194700	14.431053	-0.061072	4.704534
289.610886	7617.333717	14.436058	-0.061047	4.702186
289.417730	7609.274582	14.441063	-0.061007	4.699777
289.477514	7601.307057	14.446067	-0.061013	4.697394
289.582853	7593.265646	14.451072	-0.061029	4.694988
289.389205	7585.227331	14.456077	-0.060988	4.692581
289.628263	7577.282571	14.461082	-0.061028	4.690201
289.611046	7569.285955	14.466087	-0.061021	4.687805
289.532757	7561.230604	14.471091	-0.061002	4.685390
289.339706	7553.283833	14.476096	-0.060962	4.683006
289.513291	7545.272618	14.481101	-0.060989	4.680601
289.194128	7537.324000	14.486106	-0.060926	4.678215
289.189787	7529.226501	14.491111	-0.060921	4.675782
289.402503	7521.202892	14.496115	-0.060956	4.673369
289.403307	7513.169825	14.501120	-0.060952	4.670953
289.032441	7505.195120	14.506125	-0.060878	4.668554
289.121263	7497.194677	14.511130	-0.060890	4.666145
289.153046	7489.240563	14.516135	-0.060892	4.663749
289.037820	7481.214303	14.521139	-0.060866	4.661330
288.907820	7473.232567	14.526144	-0.060838	4.658923
289.006741	7465.220732	14.531149	-0.060852	4.656506
288.903973	7457.250535	14.536154	-0.060828	4.654100
288.976601	7449.161110	14.541159	-0.060837	4.651657
289.043427	7441.187447	14.546163	-0.060845	4.649247
289.077676	7433.254962	14.551168	-0.060847	4.646849
288.782712	7425.203845	14.556173	-0.060788	4.644414
288.848952	7417.247782	14.561178	-0.060796	4.642006
288.835355	7409.175029	14.566183	-0.060789	4.639561
288.748655	7401.247506	14.571187	-0.060769	4.637159
288.615751	7393.204592	14.576192	-0.060740	4.634721
288.473154	7385.139193	14.581197	-0.060709	4.632275
288.588186	7377.157769	14.586202	-0.060726	4.629853
288.425154	7369.145095	14.591207	-0.060691	4.627421
288.344339	7361.145037	14.596211	-0.060672	4.624990
288.454628	7353.238792	14.601216	-0.060688	4.622587
288.311185	7345.160856	14.606221	-0.060657	4.620131
288.291389	7337.212531	14.611226	-0.060649	4.617713
288.328273	7329.133077	14.616231	-0.060651	4.615253
288.253452	7321.157279	14.621235	-0.060633	4.612824
288.287486	7313.114046	14.626240	-0.060635	4.610373
288.270281	7305.136503	14.631245	-0.060627	4.607941
288.189799	7297.153989	14.636250	-0.060608	4.605505
287.974545	7289.180896	14.641255	-0.060564	4.603072
287.975737	7281.156798	14.646259	-0.060559	4.600621
288.278187	7273.191917	14.651264	-0.060611	4.598188
287.957883	7265.127593	14.656269	-0.060547	4.595722
287.913864	7257.093943	14.661274	-0.060535	4.593265
288.078815	7249.086775	14.666279	-0.060561	4.590814
288.036937	7241.107584	14.671283	-0.060549	4.588371
287.891785	7233.113487	14.676288	-0.060518	4.585922
287.848200	7225.098075	14.681293	-0.060505	4.583465
287.795922	7217.133815	14.686298	-0.060491	4.581022
287.765691	7209.150385	14.691303	-0.060481	4.578572
287.608911	7201.117683	14.696307	-0.060448	4.576106
287.552310	7193.086063	14.701312	-0.060433	4.573639
287.610039	7185.076754	14.706317	-0.060439	4.571177
287.489796	7177.129127	14.711322	-0.060412	4.568733
287.736906	7169.061865	14.716327	-0.060454	4.566251
287.564870	7161.129109	14.721331	-0.060418	4.563809
287.403765	7153.141861	14.726336	-0.060383	4.561348
287.428371	7145.112705	14.731341	-0.060384	4.558874
287.491405	7137.144431	14.736346	-0.060391	4.556417
287.261311	7129.130087	14.741351	-0.060344	4.553944
287.214468	7121.027373	14.746355	-0.060331	4.551442
287.370279	7113.086851	14.751360	-0.060355	4.548990
287.480459	7105.061899	14.756365	-0.060371	4.546510
287.331940	7097.071860	14.761370	-0.060339	4.544039
287.216061	7089.127425	14.766375	-0.060314	4.541581
287.192649	7081.119286	14.771379	-0.060305	4.539103
287.289619	7073.141064	14.776384	-0.060319	4.536632
287.133674	7065.071930	14.781389	-0.060285	4.534131
287.175173	7057.066533	14.786394	-0.060288	4.531649
286.974372	7049.066003	14.791399	-0.060247	4.529167
287.024212	7041.102535	14.796403	-0.060252	4.526695
287.090266	7033.079983	14.801408	-0.060260	4.524204
286.894615	7025.097751	14.806413	-0.060219	4.521723
287.034625	7017.090543	14.811418	-0.060241	4.519234
286.887290	7009.128882	14.816423	-0.060209	4.516757
286.845658	7001.064583	14.821427	-0.060197	4.514247
286.840203	6993.008528	14.826432	-0.060191	4.511738
286.839910	6985.012014	14.831437	-0.060187	4.509246
286.984135	6977.020783	14.836442	-0.060209	4.506755
286.751406	6969.002962	14.841447	-0.060162	4.504254
286.584094	6961.075149	14.846451	-0.060126	4.501779
286.657733	6953.018792	14.851456	-0.060136	4.499263
286.739942	6945.043757	14.856461	-0.060146	4.496771
286.565397	6937.034469	14.861466	-0.060110	4.494267
286.546616	6929.058237	14.866471	-0.060102	4.491772
286.503705	6921.014877	14.871475	-0.060089	4.489254
286.477351	6913.061606	14.876480	-0.060080	4.486763
286.352880	6905.012116	14.881485	-0.060053	4.484241
286.478925	6897.125021	14.886490	-0.060072	4.481769
286.422455	6889.026170	14.891495	-0.060057	4.479228
286.229917	6881.067583	14.896499	-0.060017	4.476729
286.356341	6873.019749	14.901504	-0.060036	4.474202
286.358077	6864.997611	14.906509	-0.060032	4.471682
286.460066	6857.022596	14.911514	-0.060046	4.469175
286.248476	6849.020753	14.916519	-0.060003	4.466657
286.219082	6840.977837	14.921523	-0.059993	4.464125
286.138343	6833.046130	14.926528	-0.059974	4.461627
285.897954	6825.008832	14.931533	-0.059924	4.459093
286.158276	6817.021769	14.936538	-0.059969	4.456576
285.964259	6808.999062	14.941543	-0.059928	4.454045
285.836953	6800.981176	14.946547	-0.059900	4.451513
285.917326	6792.969288	14.951552	-0.059911	4.448983
285.833754	6784.978809	14.956557	-0.059891	4.446458
285.714984	6777.007177	14.961562	-0.059864	4.443937
285.668174	6769.022419	14.966567	-0.059851	4.441410
285.733699	6761.001311	14.971571	-0.059859	4.438872
285.738615	6753.021057	14.976576	-0.059856	4.436344
285.641595	6744.958100	14.981581	-0.059833	4.433788
285.675364	6736.930522	14.986586	-0.059835	4.431243
285.627913	6728.971637	14.991591	-0.059822	4.428718
285.491137	6720.935012	14.996595	-0.059792	4.426166
285.491947	6712.982665	15.001600	-0.059788	4.423640
285.661487	6704.929307	15.006605	-0.059815	4.421081
285.530378	6696.994894	15.011610	-0.059786	4.418557
285.544707	6688.945200	15.016615	-0.059785	4.415996
285.519327	6680.938028	15.021619	-0.059775	4.413446
285.360136	6672.935585	15.026624	-0.059741	4.410896
285.067029	6664.952642	15.031629	-0.059683	4.408350
285.271559	6656.977396	15.036634	-0.059716	4.405808
285.302827	6648.945857	15.041639	-0.059718	4.403245
285.085378	6640.956218	15.046643	-0.059673	4.400693
285.386067	6633.007819	15.051648	-0.059725	4.398155
285.315786	6624.985057	15.056653	-0.059707	4.395590
285.301968	6616.923139	15.061658	-0.059700	4.393011
285.054600	6608.918660	15.066663	-0.059650	4.390448
285.057475	6600.930290	15.071667	-0.059646	4.387890
285.131774	6592.947302	15.076672	-0.059655	4.385332
284.989439	6584.971747	15.081677	-0.059625	4.382774
284.970177	6576.983178	15.086682	-0.059617	4.380211
284.995589	6569.000447	15.091687	-0.059617	4.377649
284.914594	6560.917409	15.096691	-0.059598	4.375053
284.811001	6552.965871	15.101696	-0.059574	4.372497
284.724747	6544.903210	15.106701	-0.059554	4.369903
284.758167	6536.982835	15.111706	-0.059555	4.367355
284.587731	6528.959416	15.116711	-0.059519	4.364771
284.489274	6520.992744	15.121715	-0.059497	4.362204
284.728933	6512.980755	15.126720	-0.059537	4.359623
284.442564	6505.003925	15.131725	-0.059479	4.357049
284.643165	6496.953742	15.136730	-0.059512	4.354452
284.663274	6488.839357	15.141735	-0.059512	4.351832
284.366915	6480.872373	15.146739	-0.059452	4.349256
284.422948	6472.906034	15.151744	-0.059458	4.346681
284.451520	6464.881279	15.156749	-0.059459	4.344086
284.646522	6456.978432	15.161754	-0.059491	4.341529
284.316014	6448.955173	15.166759	-0.059425	4.338928
284.211855	6440.940798	15.171763	-0.059401	4.336331
284.357436	6432.928891	15.176768	-0.059424	4.333734
284.210908	6424.878896	15.181773	-0.059393	4.331121
284.082204	6416.916118	15.186778	-0.059364	4.328535
284.117594	6408.926735	15.191783	-0.059366	4.325940
284.199084	6400.940169	15.196787	-0.059377	4.323345
284.198213	6392.959231	15.201792	-0.059373	4.320749
284.159479	6384.942698	15.206797	-0.059361	4.318140
283.993502	6376.932931	15.211802	-0.059326	4.315531
283.842853	6368.937313	15.216807	-0.059294	4.312924
283.928551	6360.871311	15.221811	-0.059305	4.310295
284.030694	6352.912193	15.226816	-0.059320	4.307700
283.828369	6344.897981	15.231821	-0.059278	4.305082
283.903304	6336.912813	15.236826	-0.059287	4.302475
283.875813	6328.910051	15.241831	-0.059278	4.299859
283.945738	6320.919401	15.246835	-0.059287	4.297247
283.883966	6312.912903	15.251840	-0.059271	4.294626
283.810112	6304.855375	15.256845	-0.059253	4.291988
283.833624	6296.869053	15.261850	-0.059253	4.289371
283.519033	6288.909243	15.266855	-0.059190	4.286759
283.423980	6280.860488	15.271859	-0.059168	4.284119
283.548224	6272.896843	15.276864	-0.059186	4.281506
283.435844	6264.918313	15.281869	-0.059161	4.278885
283.534927	6256.905170	15.286874	-0.059175	4.276252
283.615421	6248.888860	15.291879	-0.059186	4.273617
283.660045	6240.866061	15.296883	-0.059190	4.270977
283.662121	6232.881543	15.301888	-0.059186	4.268349
283.427919	6224.857915	15.306893	-0.059138	4.265703
283.581734	6216.881220	15.311898	-0.059162	4.263075
283.410202	6208.886794	15.316903	-0.059126	4.260437
283.389084	6200.897158	15.321907	-0.059118	4.257800
283.374318	6192.903811	15.326912	-0.059111	4.255160
283.025103	6184.881059	15.331917	-0.059041	4.252506
283.026869	6176.857655	15.336922	-0.059037	4.249852
283.024808	6168.857295	15.341927	-0.059032	4.247205
282.806856	6160.824545	15.346931	-0.058987	4.244544
282.798279	6152.926746	15.351936	-0.058982	4.241927
282.704851	6144.862980	15.356941	-0.058960	4.239253
282.830524	6136.932698	15.361946	-0.058979	4.236624
282.688762	6128.868220	15.366951	-0.058948	4.233946
282.692034	6120.833882	15.371955	-0.058944	4.231277
282.857890	6112.860028	15.376960	-0.058971	4.228629
282.802148	6104.860005	15.381965	-0.058956	4.225968
282.771609	6096.889635	15.386970	-0.058946	4.223316
282.747007	6088.907245	15.391975	-0.058937	4.220658
282.733713	6080.912702	15.396979	-0.058930	4.217994
282.639011	6072.861055	15.401984	-0.058908	4.215309
282.666709	6064.898850	15.406989	-0.058909	4.212653
282.707863	6056.857108	15.411994	-0.058912	4.209969
282.744041	6048.942103	15.416999	-0.058915	4.207325
282.496881	6040.885725	15.422003	-0.058864	4.204630
282.762337	6032.958812	15.427008	-0.058910	4.201982
282.668097	6024.932299	15.432013	-0.058888	4.199295
282.492154	6016.962909	15.437018	-0.058851	4.196624
282.480001	6008.859413	15.442023	-0.058844	4.193909
282.534630	6000.777684	15.447027	-0.058850	4.191199
282.231964	5992.853898	15.452032	-0.058789	4.188538
282.246148	5984.822900	15.457037	-0.058787	4.185841
282.265449	5976.887023	15.462042	-0.058787	4.183175
282.128882	5968.887901	15.467047	-0.058757	4.180485
282.222026	5960.880022	15.472051	-0.058770	4.177792
282.362275	5952.894277	15.477056	-0.058792	4.175106
282.133040	5944.851655	15.482061	-0.058744	4.172394
282.043732	5936.868065	15.487066	-0.058723	4.169702
282.273899	5928.873480	15.492071	-0.058762	4.167009
282.193012	5920.812091	15.497075	-0.058743	4.164287
282.144050	5912.940694	15.502080	-0.058729	4.161629
282.004598	5904.889932	15.507085	-0.058699	4.158907
281.928403	5896.894957	15.512090	-0.058680	4.156202
281.829896	5888.852490	15.517095	-0.058658	4.153480
281.900515	5880.805826	15.522099	-0.058666	4.150756
281.911027	5872.873357	15.527104	-0.058664	4.148069
281.873302	5864.845530	15.532109	-0.058653	4.145347
281.691444	5856.911765	15.537114	-0.058614	4.142653
281.691313	5848.876626	15.542119	-0.058610	4.139925
281.666071	5840.889941	15.547123	-0.058601	4.137212
281.667292	5832.872678	15.552128	-0.058597	4.134487
281.472425	5824.831031	15.557133	-0.058556	4.131749
281.446854	5816.840967	15.562138	-0.058547	4.129029
281.625900	5808.848773	15.567143	-0.058576	4.126309
281.456250	5800.885464	15.572147	-0.058540	4.123593
281.406570	5792.859944	15.577152	-0.058526	4.120856
281.407727	5784.853460	15.582157	-0.058522	4.118123
281.320571	5776.891203	15.587162	-0.058502	4.115403
281.189073	5768.850966	15.592167	-0.058473	4.112654
281.067550	5760.797539	15.597171	-0.058446	4.109898
281.159475	5752.861027	15.602176	-0.058459	4.107184
280.923744	5744.832731	15.607181	-0.058410	4.104432
281.127501	5736.898897	15.612186	-0.058444	4.101716
281.164952	5728.874639	15.617191	-0.058447	4.098965
280.937919	5720.861350	15.622195	-0.058400	4.096213
281.007456	5712.883931	15.627200	-0.058409	4.093475
281.036511	5704.833457	15.632205	-0.058410	4.090709
280.830899	5696.890147	15.637210	-0.058367	4.087976
280.815938	5688.840460	15.642215	-0.058360	4.085206
280.734338	5680.900395	15.647219	-0.058340	4.082472
281.038926	5672.900608	15.652224	-0.058393	4.079720
280.641742	5664.930334	15.657229	-0.058314	4.076967
280.800939	5656.905421	15.662234	-0.058340	4.074201
280.735112	5648.875029	15.667239	-0.058323	4.071428
280.606854	5640.867110	15.672243	-0.058295	4.068660
280.563940	5632.891942	15.677248	-0.058283	4.065902
280.594889	5624.906572	15.682253	-0.058284	4.063141
280.519285	5616.884995	15.687258	-0.058266	4.060363
280.494440	5608.927228	15.692263	-0.058257	4.057606
280.453846	5600.865687	15.697267	-0.058245	4.054812
280.372854	5592.923871	15.702272	-0.058225	4.052056
280.239363	5584.891675	15.707277	-0.058196	4.049266
280.294286	5576.905714	15.712282	-0.058202	4.046493
280.522381	5568.911649	15.717287	-0.058240	4.043718
280.291069	5560.930710	15.722291	-0.058193	4.040939
280.285762	5552.944883	15.727296	-0.058187	4.038159
280.297391	5544.902908	15.732301	-0.058185	4.035358
280.240948	5536.811228	15.737306	-0.058170	4.032537
280.218881	5528.823084	15.742311	-0.058162	4.029751
280.173977	5520.847725	15.747315	-0.058149	4.026967
280.141190	5512.868445	15.752320	-0.058139	4.024179
279.945688	5504.903588	15.757325	-0.058098	4.021393
279.884552	5496.887596	15.762330	-0.058082	4.018588
279.942657	5488.913006	15.767335	-0.058089	4.015798
279.821134	5480.852072	15.772339	-0.058062	4.012973
279.833584	5472.845245	15.777344	-0.058059	4.010167
279.827188	5464.870667	15.782349	-0.058054	4.007370
279.781108	5456.857202	15.787354	-0.058041	4.004557
279.632618	5448.941073	15.792359	-0.058009	4.001774
279.606820	5440.881134	15.797363	-0.058000	3.998941
279.688351	5432.942735	15.802368	-0.058011	3.996150
279.425612	5424.876555	15.807373	-0.057957	3.993307
279.527120	5416.821740	15.812378	-0.057972	3.990471
279.693228	5408.858191	15.817383	-0.057999	3.987667
279.531756	5400.833875	15.822387	-0.057964	3.984834
279.581747	5392.901925	15.827392	-0.057969	3.982035
279.454382	5384.878638	15.832397	-0.057941	3.979199
279.470396	5376.916242	15.837402	-0.057940	3.976385
279.286984	5368.902655	15.842407	-0.057901	3.973548
279.104674	5360.858676	15.847411	-0.057863	3.970697
279.392177	5352.889980	15.852416	-0.057912	3.967879
279.126945	5344.877341	15.857421	-0.057858	3.965035
278.946140	5336.942207	15.862426	-0.057820	3.962217
279.042213	5328.928345	15.867431	-0.057834	3.959373
279.129806	5320.949602	15.872435	-0.057846	3.956541
279.053872	5312.917710	15.877440	-0.057827	3.953684
278.943256	5304.876671	15.882445	-0.057802	3.950821
279.103930	5296.894070	15.887450	-0.057828	3.947982
278.885136	5288.929535	15.892455	-0.057783	3.945141
278.811575	5280.915577	15.897459	-0.057765	3.942282
279.106330	5272.940957	15.902464	-0.057815	3.939442
278.739506	5264.971424	15.907469	-0.057743	3.936590
278.801633	5256.948131	15.912474	-0.057750	3.933725
278.809819	5248.916765	15.917479	-0.057747	3.930853
278.713926	5240.943566	15.922483	-0.057725	3.927998
278.663199	5232.947798	15.927488	-0.057711	3.925134
278.513153	5224.967247	15.932493	-0.057679	3.922272
278.464756	5216.956996	15.937498	-0.057665	3.919398
278.452205	5209.019523	15.942503	-0.057659	3.916549
278.367053	5200.949026	15.947507	-0.057638	3.913649
278.352873	5192.952992	15.952512	-0.057632	3.910775
278.340211	5184.935005	15.957517	-0.057625	3.907891
278.331112	5176.924498	15.962522	-0.057619	3.905008
278.556699	5168.996153	15.967527	-0.057656	3.902156
278.485010	5160.933972	15.972531	-0.057639	3.899248
278.340284	5152.997567	15.977536	-0.057607	3.896383
278.144829	5144.944375	15.982541	-0.057567	3.893472
278.330592	5136.911839	15.987546	-0.057597	3.890573
278.268105	5128.975112	15.992551	-0.057581	3.887703
278.002211	5120.956705	15.997555	-0.057527	3.884796
278.181104	5112.993214	16.002560	-0.057556	3.881916
278.012120	5104.981743	16.007565	-0.057520	3.879010
277.959287	5097.011454	16.012570	-0.057506	3.876119
277.976325	5088.838726	16.017575	-0.057505	3.873153
278.075808	5080.726248	16.022579	-0.057519	3.870209
277.932913	5072.873417	16.027584	-0.057488	3.867352
277.784127	5064.869760	16.032589	-0.057456	3.864438
277.833963	5056.922272	16.037594	-0.057461	3.861546
277.770361	5048.944938	16.042599	-0.057445	3.858639
277.760457	5040.939887	16.047603	-0.057438	3.855720
277.785324	5032.962945	16.052608	-0.057439	3.852810
277.912609	5024.916282	16.057613	-0.057458	3.849875
277.932217	5016.952559	16.062618	-0.057457	3.846966
277.838260	5008.957642	16.067623	-0.057436	3.844040
277.719768	5000.981311	16.072627	-0.057409	3.841119
277.685901	4993.011481	16.077632	-0.057399	3.838200
277.551756	4984.993760	16.082637	-0.057369	3.835259
277.609987	4976.983323	16.087642	-0.057376	3.832322
277.631353	4968.988743	16.092647	-0.057375	3.829388
277.425484	4960.976649	16.097651	-0.057333	3.826440
277.392166	4953.014476	16.102656	-0.057322	3.823512
277.410408	4944.991860	16.107661	-0.057321	3.820561
277.239782	4937.075259	16.112666	-0.057285	3.817643
277.139219	4929.051508	16.117671	-0.057262	3.814684
277.318944	4921.000086	16.122675	-0.057291	3.811719
277.299667	4913.038253	16.127680	-0.057283	3.808780
277.301545	4904.997700	16.132685	-0.057279	3.805810
277.269798	4897.073454	16.137690	-0.057269	3.802881
277.221906	4889.053355	16.142695	-0.057256	3.799913
277.085088	4881.081011	16.147699	-0.057226	3.796958
277.209440	4873.049024	16.152704	-0.057245	3.793985
276.985634	4865.011863	16.157709	-0.057199	3.791000
276.645205	4857.001501	16.162714	-0.057131	3.788020
276.793990	4849.017249	16.167719	-0.057154	3.785059
276.762294	4841.040715	16.172723	-0.057144	3.782093
276.845569	4833.082872	16.177728	-0.057155	3.779135
276.509623	4825.064177	16.182733	-0.057088	3.776143
276.623005	4817.060111	16.187738	-0.057105	3.773163
276.634796	4809.046699	16.192743	-0.057103	3.770176
276.531911	4801.064986	16.197747	-0.057079	3.767195
276.588455	4793.057383	16.202752	-0.057085	3.764206
276.738594	4785.075462	16.207757	-0.057109	3.761227
276.545659	4777.095767	16.212762	-0.057069	3.758238
276.655316	4769.063084	16.217767	-0.057085	3.755234
276.574838	4761.019339	16.222771	-0.057065	3.752218
276.602222	4753.034532	16.227776	-0.057066	3.749225
276.517364	4745.029783	16.232781	-0.057046	3.746220
276.521428	4737.053394	16.237786	-0.057042	3.743224
276.492357	4729.075495	16.242791	-0.057033	3.740225
276.148543	4721.118718	16.247795	-0.056964	3.737225
276.197121	4713.089156	16.252800	-0.056969	3.734203
276.321887	4705.088615	16.257805	-0.056988	3.731192
276.256648	4697.084958	16.262810	-0.056971	3.728173
276.111780	4689.099475	16.267815	-0.056940	3.725156
276.212190	4681.118997	16.272819	-0.056954	3.722144
276.037925	4673.134366	16.277824	-0.056918	3.719122
276.092447	4665.173034	16.282829	-0.056923	3.716112
276.060127	4657.090164	16.287834	-0.056913	3.713051
276.057967	4649.035924	16.292839	-0.056908	3.709999
275.791542	4641.064607	16.297843	-0.056854	3.706970
275.749483	4633.062394	16.302848	-0.056842	3.703932
275.977016	4625.101861	16.307853	-0.056880	3.700914
275.742630	4617.145764	16.312858	-0.056832	3.697884
275.701538	4609.144312	16.317863	-0.056820	3.694839
275.590072	4601.159001	16.322867	-0.056795	3.691795
275.725105	4593.159234	16.327872	-0.056816	3.688750
275.694896	4585.162169	16.332877	-0.056806	3.685699
275.696880	4577.173704	16.337882	-0.056802	3.682650
275.668823	4569.190582	16.342887	-0.056792	3.679600
275.339969	4561.248764	16.347891	-0.056727	3.676555
275.390117	4553.197096	16.352896	-0.056732	3.673475
275.438490	4545.158800	16.357901	-0.056736	3.670397
275.341887	4537.201255	16.362906	-0.056714	3.667345
275.192815	4529.196968	16.367911	-0.056682	3.664270
275.357293	4521.205162	16.372915	-0.056708	3.661206
275.522342	4513.215067	16.377920	-0.056735	3.658140
275.306413	4505.210360	16.382925	-0.056690	3.655056
275.218827	4497.198922	16.387930	-0.056669	3.651970
275.252110	4489.205502	16.392935	-0.056671	3.648891
275.142658	4481.191345	16.397939	-0.056647	3.645798
275.019148	4473.241608	16.402944	-0.056619	3.642727
274.911754	4465.223196	16.407949	-0.056595	3.639627
274.865009	4457.264801	16.412954	-0.056582	3.636549
274.896651	4449.231126	16.417959	-0.056583	3.633442
274.736565	4441.192621	16.422963	-0.056549	3.630325
274.820123	4433.221457	16.427968	-0.056560	3.627238
274.725979	4425.212313	16.432973	-0.056538	3.624129
274.636656	4417.225827	16.437978	-0.056518	3.621026
274.630287	4409.243628	16.442983	-0.056512	3.617924
274.495886	4401.224321	16.447987	-0.056483	3.614802
274.727121	4393.261599	16.452992	-0.056521	3.611709
274.618138	4385.263156	16.457997	-0.056497	3.608590
274.756170	4377.259778	16.463002	-0.056518	3.605473
274.520333	4369.306622	16.468007	-0.056470	3.602363
274.321814	4361.297863	16.473011	-0.056428	3.599230
274.503224	4353.348853	16.478016	-0.056458	3.596127
274.333501	4345.308954	16.483021	-0.056422	3.592977
274.369197	4337.277369	16.488026	-0.056424	3.589833
274.559677	4329.326849	16.493031	-0.056455	3.586722
274.327206	4321.332551	16.498035	-0.056408	3.583579
274.268593	4313.366960	16.503040	-0.056392	3.580450
274.175951	4305.370335	16.508045	-0.056371	3.577305
274.092898	4297.358670	16.513050	-0.056351	3.574151
274.094375	4289.343190	16.518055	-0.056347	3.570996
273.950398	4281.335147	16.523059	-0.056316	3.567837
274.059268	4273.355276	16.528064	-0.056332	3.564693
273.985785	4265.401349	16.533069	-0.056314	3.561551
273.838759	4257.388815	16.538074	-0.056282	3.558381
273.892493	4249.420726	16.543079	-0.056288	3.555232
273.830036	4241.310602	16.548083	-0.056272	3.552020
274.034423	4233.301439	16.553088	-0.056305	3.548854
273.773421	4225.330092	16.558093	-0.056252	3.545686
273.756201	4217.379226	16.563098	-0.056245	3.542530
273.641368	4209.383061	16.568103	-0.056219	3.539350
273.574464	4201.398386	16.573107	-0.056202	3.536174
273.676879	4193.383856	16.578112	-0.056217	3.532988
273.564950	4185.388780	16.583117	-0.056192	3.529801
273.497253	4177.406242	16.588122	-0.056175	3.526616
273.538338	4169.414089	16.593127	-0.056178	3.523429
273.473069	4161.411460	16.598131	-0.056162	3.520231
273.431687	4153.477547	16.603136	-0.056150	3.517058
273.330655	4145.468022	16.608141	-0.056127	3.513851
273.484167	4137.420629	16.613146	-0.056151	3.510633
273.450184	4129.431550	16.618151	-0.056140	3.507430
273.337151	4121.422433	16.623155	-0.056115	3.504213
273.277961	4113.494276	16.628160	-0.056099	3.501028
273.313349	4105.490730	16.633165	-0.056102	3.497812
273.102340	4097.495044	16.638170	-0.056058	3.494589
273.310239	4089.492830	16.643175	-0.056092	3.491373
273.086269	4081.495203	16.648179	-0.056046	3.488143
272.872069	4073.512836	16.653184	-0.056002	3.484916
272.944658	4065.539432	16.658189	-0.056011	3.481699
273.062776	4057.529642	16.663194	-0.056029	3.478465
272.940339	4049.580143	16.668199	-0.056002	3.475246
272.701893	4041.541656	16.673203	-0.055953	3.471983
272.717730	4033.517649	16.678208	-0.055951	3.468732
272.852348	4025.524040	16.683213	-0.055972	3.465493
272.686221	4017.557163	16.688218	-0.055937	3.462253
272.571936	4009.569121	16.693223	-0.055911	3.459003
272.801498	4001.552713	16.698227	-0.055950	3.455749
272.569086	3993.579247	16.703232	-0.055902	3.452494
272.401597	3985.552306	16.708237	-0.055867	3.449217
272.632937	3977.574378	16.713242	-0.055905	3.445970
272.753687	3969.583758	16.718247	-0.055923	3.442711
272.502833	3961.632250	16.723251	-0.055872	3.439453
272.507099	3953.665413	16.728256	-0.055869	3.436193
272.496928	3945.639497	16.733261	-0.055863	3.432906
272.563903	3937.563225	16.738266	-0.055871	3.429598
272.505960	3929.645613	16.743271	-0.055856	3.426347
272.274280	3921.635048	16.748275	-0.055808	3.423049
272.290135	3913.658294	16.753280	-0.055807	3.419771
272.248801	3905.665835	16.758285	-0.055795	3.416480
272.224656	3897.657710	16.763290	-0.055786	3.413181
272.123599	3889.647807	16.768295	-0.055763	3.409875
271.966378	3881.681375	16.773299	-0.055729	3.406582
272.085272	3873.689216	16.778304	-0.055747	3.403285
272.093296	3865.711715	16.783309	-0.055744	3.399986
272.075402	3857.751655	16.788314	-0.055736	3.396691
272.140204	3849.689987	16.793319	-0.055744	3.393353
271.895520	3841.644860	16.798323	-0.055694	3.390008
271.857056	3833.685926	16.803328	-0.055683	3.386703
271.775230	3825.727921	16.808333	-0.055663	3.383393
271.549993	3817.740336	16.813338	-0.055617	3.380063
271.694905	3809.777381	16.818343	-0.055639	3.376753
271.761523	3801.765916	16.823347	-0.055647	3.373416
271.551048	3793.774678	16.828352	-0.055604	3.370075
271.497301	3785.781105	16.833357	-0.055589	3.366735
271.365585	3777.780501	16.838362	-0.055561	3.363386
271.355735	3769.827466	16.843367	-0.055554	3.360058
271.281135	3761.833486	16.848371	-0.055536	3.356707
271.440604	3753.813267	16.853376	-0.055562	3.353351
271.420010	3745.800903	16.858381	-0.055553	3.349987
271.543437	3737.793819	16.863386	-0.055572	3.346628
271.487457	3729.854022	16.868391	-0.055557	3.343287
271.341727	3721.838057	16.873395	-0.055526	3.339908
271.234041	3713.895837	16.878400	-0.055501	3.336557
271.329970	3705.863277	16.883405	-0.055515	3.333172
271.004190	3697.843873	16.888410	-0.055450	3.329774
271.085937	3689.888696	16.893415	-0.055461	3.326415
270.988556	3681.906340	16.898419	-0.055438	3.323034
271.059018	3673.896775	16.903424	-0.055447	3.319645
270.886423	3665.981535	16.908429	-0.055411	3.316283
270.800298	3657.934429	16.913434	-0.055390	3.312864
270.870989	3649.911913	16.918439	-0.055399	3.309459
270.630845	3641.924448	16.923443	-0.055350	3.306053
270.606191	3633.964297	16.928448	-0.055341	3.302664
270.619952	3625.949602	16.933453	-0.055339	3.299249
270.564134	3617.978668	16.938458	-0.055324	3.295846
270.535856	3610.006223	16.943463	-0.055315	3.292441
270.532494	3601.973385	16.948467	-0.055310	3.289007
270.572076	3594.006333	16.953472	-0.055313	3.285599
270.652062	3586.022768	16.958477	-0.055323	3.282183
270.518478	3578.047098	16.963482	-0.055294	3.278757
270.573751	3570.088198	16.968487	-0.055300	3.275343
270.485937	3562.037257	16.973491	-0.055279	3.271880
270.314053	3554.068524	16.978496	-0.055243	3.268446
270.463269	3546.050779	16.983501	-0.055267	3.264999
270.228586	3538.112622	16.988506	-0.055219	3.261568
270.330886	3530.078392	16.993511	-0.055233	3.258105
270.213197	3522.097356	16.998515	-0.055207	3.254653
270.238231	3514.087941	17.003520	-0.055207	3.251190
270.162160	3506.110039	17.008525	-0.055189	3.247734
269.997303	3498.124370	17.013530	-0.055154	3.244266
270.006293	3490.178017	17.018535	-0.055151	3.240819
269.904585	3482.189289	17.023539	-0.055128	3.237346
269.790827	3474.178009	17.028544	-0.055102	3.233858
269.934371	3466.104206	17.033549	-0.055125	3.230350
269.975226	3458.118130	17.038554	-0.055128	3.226872
269.819613	3450.171136	17.043559	-0.055095	3.223399
269.658743	3442.191830	17.048563	-0.055060	3.219909
269.659576	3434.240369	17.053568	-0.055056	3.216433
269.625818	3426.216615	17.058573	-0.055045	3.212920
269.554213	3418.190257	17.063578	-0.055028	3.209401
269.720469	3410.222173	17.068583	-0.055054	3.205914
269.630880	3402.259131	17.073587	-0.055033	3.202414
269.347020	3394.313997	17.078592	-0.054976	3.198910
269.385116	3386.307463	17.083597	-0.054979	3.195389
269.443389	3378.277360	17.088602	-0.054985	3.191854
269.316736	3370.342369	17.093607	-0.054957	3.188350
269.224150	3362.307606	17.098611	-0.054936	3.184799
269.327588	3354.330175	17.103616	-0.054951	3.181277
269.330581	3346.338006	17.108621	-0.054947	3.177741
269.007484	3338.375473	17.113626	-0.054882	3.174201
269.304000	3330.346899	17.118631	-0.054933	3.170653
269.268784	3322.365467	17.123635	-0.054922	3.167108
269.150238	3314.412270	17.128640	-0.054896	3.163569
268.873002	3306.430798	17.133645	-0.054840	3.160006
268.807692	3298.454727	17.138650	-0.054824	3.156450
268.775532	3290.453670	17.143655	-0.054813	3.152881
268.559454	3282.416699	17.148659	-0.054769	3.149283
268.801750	3274.422487	17.153664	-0.054809	3.145721
268.780224	3266.451842	17.158669	-0.054801	3.142153
268.573253	3258.477779	17.163674	-0.054758	3.138572
268.703061	3250.481263	17.168679	-0.054778	3.134991
268.607421	3242.480547	17.173683	-0.054756	3.131395
268.483536	3234.518229	17.178688	-0.054728	3.127810
268.419410	3226.548109	17.183693	-0.054712	3.124220
268.601034	3218.537948	17.188698	-0.054742	3.120619
268.418502	3210.609688	17.193703	-0.054703	3.117035
268.377867	3202.574989	17.198707	-0.054691	3.113405
268.473444	3194.575467	17.203712	-0.054705	3.109792
268.644767	3186.574195	17.208717	-0.054732	3.106178
268.288156	3178.628679	17.213722	-0.054662	3.102561
268.501375	3170.625961	17.218727	-0.054697	3.098940
268.312486	3162.657693	17.223731	-0.054658	3.095312
268.235773	3154.675931	17.228736	-0.054639	3.091679
268.230447	3146.665571	17.233741	-0.054634	3.088031
268.110646	3138.651582	17.238746	-0.054607	3.084373
268.254056	3130.713543	17.243751	-0.054629	3.080756
267.910637	3122.763700	17.248755	-0.054561	3.077108
268.044674	3114.704110	17.253760	-0.054582	3.073427
267.995601	3106.669988	17.258765	-0.054568	3.069745
267.828964	3098.706485	17.263770	-0.054533	3.066085
267.974030	3090.737091	17.268775	-0.054555	3.062433
267.830229	3082.761173	17.273779	-0.054524	3.058760
267.825076	3074.783426	17.278784	-0.054519	3.055088
267.745531	3066.795141	17.283789	-0.054500	3.051404
267.690896	3058.778143	17.288794	-0.054485	3.047703
267.771425	3050.833997	17.293799	-0.054496	3.044037
267.625876	3042.855910	17.298803	-0.054465	3.040341
267.707104	3034.899201	17.303808	-0.054475	3.036661
267.686019	3026.900100	17.308813	-0.054467	3.032951
267.459947	3018.874253	17.313818	-0.054421	3.029215
267.586492	3010.904352	17.318823	-0.054440	3.025517
267.520812	3002.936652	17.323827	-0.054423	3.021807
267.423193	2994.977415	17.328832	-0.054401	3.018094
267.185717	2986.983778	17.333837	-0.054352	3.014354
267.131148	2978.970345	17.338842	-0.054338	3.010609
267.319457	2970.996145	17.343847	-0.054368	3.006889
267.166737	2963.016241	17.348851	-0.054336	3.003146
267.120405	2955.037162	17.353856	-0.054323	2.999403
267.064777	2947.101617	17.358861	-0.054308	2.995676
266.940100	2939.051161	17.363866	-0.054280	2.991886
267.257225	2931.055035	17.368871	-0.054335	2.988140
267.122497	2923.054446	17.373875	-0.054306	2.984364
267.069963	2915.110874	17.378880	-0.054292	2.980614
266.882214	2907.168597	17.383885	-0.054252	2.976853
266.877685	2899.132478	17.388890	-0.054247	2.973052
266.987814	2891.137212	17.393895	-0.054263	2.969272
266.721569	2883.181821	17.398899	-0.054209	2.965486
266.822547	2875.211156	17.403904	-0.054224	2.961707
266.764573	2867.249961	17.408909	-0.054209	2.957920
266.500535	2859.262826	17.413914	-0.054155	2.954105
266.493060	2851.259802	17.418919	-0.054149	2.950291
266.470435	2843.273996	17.423923	-0.054141	2.946479
266.498269	2835.287853	17.428928	-0.054142	2.942664
266.517269	2827.318223	17.433933	-0.054141	2.938852
266.397455	2819.330360	17.438938	-0.054114	2.935019
266.571492	2811.332092	17.443943	-0.054142	2.931192
266.263392	2803.359033	17.448947	-0.054081	2.927346
266.156097	2795.394805	17.453952	-0.054056	2.923510
266.309796	2787.413846	17.458957	-0.054081	2.919675
266.286509	2779.437444	17.463962	-0.054072	2.915827
266.366386	2771.380144	17.468967	-0.054082	2.911941
266.137011	2763.384969	17.473971	-0.054035	2.908063
266.028987	2755.419437	17.478976	-0.054011	2.904201
265.964617	2747.481621	17.483981	-0.053995	2.900349
265.765650	2739.518483	17.488986	-0.053953	2.896473
265.923381	2731.500956	17.493991	-0.053978	2.892584
265.919618	2723.515235	17.498995	-0.053973	2.888697
265.756220	2715.547114	17.504000	-0.053938	2.884804
265.898019	2707.582721	17.509005	-0.053960	2.880925
265.737884	2699.617948	17.514010	-0.053926	2.877024
265.645642	2691.649468	17.519015	-0.053905	2.873119
265.499534	2683.651422	17.524019	-0.053873	2.869192
265.585494	2675.637767	17.529024	-0.053885	2.865264
265.699042	2667.690998	17.534029	-0.053902	2.861365
265.409399	2659.706494	17.539034	-0.053843	2.857420
265.551878	2651.735156	17.544039	-0.053866	2.853500
265.472107	2643.721366	17.549043	-0.053846	2.849541
265.396461	2635.764376	17.554048	-0.053828	2.845606
265.393835	2627.805755	17.559053	-0.053823	2.841667
265.296309	2619.827371	17.564058	-0.053801	2.837709
265.379001	2611.826499	17.569063	-0.053812	2.833743
264.985235	2603.860223	17.574067	-0.053734	2.829763
265.219303	2595.836323	17.579072	-0.053773	2.825784
265.129313	2587.898153	17.584077	-0.053752	2.821823
265.043752	2579.914401	17.589082	-0.053732	2.817834
264.898824	2571.968776	17.594087	-0.053701	2.813856
264.903938	2563.939322	17.599091	-0.053697	2.809838
264.896225	2555.974491	17.604096	-0.053691	2.805846
264.905851	2548.018377	17.609101	-0.053689	2.801854
264.879878	2540.038592	17.614106	-0.053680	2.797842
264.688892	2532.085605	17.619111	-0.053640	2.793829
264.730412	2524.051638	17.624115	-0.053643	2.789782
264.840215	2516.067124	17.629120	-0.053659	2.785758
264.673464	2508.128655	17.634125	-0.053624	2.781736
264.576154	2500.148695	17.639130	-0.053602	2.777691
264.461286	2492.184917	17.644135	-0.053576	2.773647
264.389530	2484.179241	17.649139	-0.053558	2.769578
264.216804	2476.241341	17.654144	-0.053522	2.765532
264.270124	2468.264184	17.659149	-0.053527	2.761473
264.089496	2460.308410	17.664154	-0.053489	2.757406
264.222818	2452.281178	17.669159	-0.053510	2.753314
264.178067	2444.224533	17.674163	-0.053497	2.749191
264.214202	2436.254510	17.679168	-0.053499	2.745111
264.289562	2428.320264	17.684173	-0.053509	2.741046
264.102079	2420.362021	17.689178	-0.053470	2.736946
264.124926	2412.386050	17.694183	-0.053470	2.732843
263.965707	2404.391567	17.699187	-0.053436	2.728714
263.903025	2396.428026	17.704192	-0.053420	2.724601
263.961316	2388.482670	17.709197	-0.053426	2.720498
263.931669	2380.497069	17.714202	-0.053416	2.716362
263.902634	2372.516347	17.719207	-0.053407	2.712223
263.862551	2364.533520	17.724211	-0.053395	2.708076
263.726900	2356.579183	17.729216	-0.053365	2.703931
263.776602	2348.602904	17.734221	-0.053370	2.699780
263.440326	2340.670878	17.739226	-0.053303	2.695622
263.512715	2332.679412	17.744231	-0.053312	2.691451
263.630383	2324.656079	17.749235	-0.053330	2.687261
263.279135	2316.735129	17.754240	-0.053260	2.683087
263.297891	2308.782555	17.759245	-0.053259	2.678915
263.285559	2300.782630	17.764250	-0.053253	2.674708
263.289290	2292.774384	17.769255	-0.053249	2.670492
263.099059	2284.815355	17.774259	-0.053209	2.666283
263.238822	2276.826483	17.779264	-0.053231	2.662072
263.400061	2268.846957	17.784269	-0.053257	2.657861
262.946849	2260.910831	17.789274	-0.053168	2.653627
262.996903	2252.893773	17.794279	-0.053173	2.649375
263.026237	2244.935804	17.799283	-0.053174	2.645147
262.805786	2237.003010	17.804288	-0.053129	2.640909
262.895816	2229.046394	17.809293	-0.053141	2.636672
262.890738	2221.024862	17.814298	-0.053136	2.632387
263.122653	2213.025082	17.819303	-0.053175	2.628122
262.774735	2205.103304	17.824307	-0.053106	2.623854
262.932325	2197.110915	17.829312	-0.053131	2.619575
262.727648	2189.184751	17.834317	-0.053088	2.615300
262.270350	2181.218708	17.839322	-0.052999	2.610979
262.221314	2173.263696	17.844327	-0.052985	2.606685
262.412032	2165.252448	17.849331	-0.053016	2.602369
262.318141	2157.320948	17.854336	-0.052995	2.598070
262.411932	2149.277940	17.859341	-0.053008	2.593717
262.247154	2141.157762	17.864346	-0.052973	2.589296
262.230478	2133.246036	17.869351	-0.052965	2.584991
262.225298	2125.298534	17.874355	-0.052960	2.580661
262.410546	2117.330747	17.879360	-0.052990	2.576325
262.285261	2109.401606	17.884365	-0.052962	2.571982
261.950023	2101.457400	17.889370	-0.052896	2.567608
261.971469	2093.499849	17.894375	-0.052895	2.563245
262.092478	2085.524805	17.899379	-0.052914	2.558871
261.855588	2077.580824	17.904384	-0.052865	2.554482
261.808872	2069.591747	17.909389	-0.052852	2.550073
261.755141	2061.608360	17.914394	-0.052838	2.545660
261.792153	2053.672126	17.919399	-0.052840	2.541272
261.674005	2045.724862	17.924403	-0.052814	2.536859
261.760363	2037.732277	17.929408	-0.052826	2.532427
261.830468	2029.757379	17.934413	-0.052834	2.527996
261.561912	2021.818437	17.939418	-0.052780	2.523554
261.545375	2013.867228	17.944423	-0.052773	2.519115
261.610876	2005.897761	17.949427	-0.052781	2.514664
261.552266	1997.878669	17.954432	-0.052765	2.510168
261.526770	1989.919737	17.959437	-0.052756	2.505700
261.585301	1981.935886	17.964442	-0.052763	2.501216
261.633451	1973.998662	17.969447	-0.052767	2.496749
261.400467	1966.053875	17.974451	-0.052720	2.492250
261.359027	1958.076710	17.979456	-0.052708	2.487739
261.357492	1950.128141	17.984461	-0.052703	2.483238
261.203469	1942.176100	17.989466	-0.052670	2.478716
261.053063	1934.238735	17.994471	-0.052638	2.474194
261.120706	1926.218556	17.999475	-0.052646	2.469633
261.064105	1918.261873	18.004480	-0.052631	2.465091
261.049792	1910.326369	18.009485	-0.052624	2.460555
260.881885	1902.366466	18.014490	-0.052589	2.455985
261.033329	1894.386184	18.019495	-0.052612	2.451420
260.813174	1886.428684	18.024499	-0.052567	2.446831
260.768399	1878.483797	18.029504	-0.052555	2.442253
260.744628	1870.548356	18.034509	-0.052546	2.437674
260.684962	1862.531633	18.039514	-0.052530	2.433037
260.511166	1854.525345	18.044519	-0.052494	2.428388
260.552234	1846.560676	18.049523	-0.052497	2.423771
260.531306	1838.613712	18.054528	-0.052489	2.419151
260.575167	1830.674422	18.059533	-0.052493	2.414531
260.291643	1822.708192	18.064538	-0.052435	2.409861
260.416885	1814.751281	18.069543	-0.052454	2.405220
260.125258	1806.832090	18.074547	-0.052396	2.400559
260.107302	1798.882158	18.079552	-0.052388	2.395892
260.136351	1790.885752	18.084557	-0.052389	2.391192
260.010150	1782.926309	18.089562	-0.052361	2.386493
260.056350	1774.969845	18.094567	-0.052366	2.381800
260.081194	1767.014747	18.099571	-0.052366	2.377097
260.123227	1759.043588	18.104576	-0.052369	2.372376
259.941798	1751.114876	18.109581	-0.052331	2.367653
259.788905	1743.169161	18.114586	-0.052299	2.362913
259.961848	1735.198958	18.119591	-0.052326	2.358175
259.757108	1727.268482	18.124595	-0.052284	2.353420
259.609895	1719.279435	18.129600	-0.052252	2.348626
259.784773	1711.295419	18.134605	-0.052280	2.343851
259.636431	1703.352162	18.139610	-0.052249	2.339064
259.424869	1695.447034	18.144615	-0.052205	2.334285
259.670113	1687.426368	18.149619	-0.052246	2.329465
259.385613	1679.499400	18.154624	-0.052189	2.324647
259.388577	1671.567861	18.159629	-0.052185	2.319840
259.337923	1663.618730	18.164634	-0.052171	2.315008
259.423444	1655.633010	18.169639	-0.052183	2.310155
259.188971	1647.694513	18.174643	-0.052135	2.305294
259.136861	1639.749432	18.179648	-0.052121	2.300434
259.107770	1631.814693	18.184653	-0.052111	2.295572
258.991646	1623.827950	18.189658	-0.052085	2.290660
259.052440	1615.886010	18.194663	-0.052092	2.285780
258.974893	1607.955510	18.199667	-0.052074	2.280885
258.972616	1600.001896	18.204672	-0.052069	2.275972
258.797438	1592.016307	18.209677	-0.052032	2.271013
258.749785	1584.025332	18.214682	-0.052019	2.266051
258.861891	1576.078875	18.219687	-0.052035	2.261120
258.811633	1568.151184	18.224691	-0.052021	2.256175
258.618643	1560.194572	18.229696	-0.051981	2.251189
258.595830	1552.254931	18.234701	-0.051973	2.246218
258.651866	1544.287576	18.239706	-0.051979	2.241225
258.617301	1536.374869	18.244711	-0.051968	2.236247
258.482518	1528.419812	18.249715	-0.051939	2.231223
258.552209	1520.450918	18.254720	-0.051947	2.226196
258.543606	1512.523246	18.259725	-0.051941	2.221178
258.356800	1504.596221	18.264730	-0.051902	2.216132
258.337477	1496.640037	18.269735	-0.051894	2.211072
258.181221	1488.712284	18.274739	-0.051861	2.206005
258.021525	1480.786722	18.279744	-0.051827	2.200928
258.065066	1472.848912	18.284749	-0.051831	2.195850
257.926954	1464.864468	18.289754	-0.051801	2.190713
257.927033	1456.903752	18.294759	-0.051796	2.185593
257.840406	1448.977830	18.299763	-0.051776	2.180474
257.901313	1441.018505	18.304768	-0.051783	2.175336
257.690381	1433.098258	18.309773	-0.051739	2.170186
257.534800	1425.164579	18.314778	-0.051706	2.165020
257.561643	1417.222262	18.319783	-0.051707	2.159853
257.686304	1409.273964	18.324787	-0.051726	2.154678
257.260731	1401.345548	18.329792	-0.051642	2.149453
257.394290	1393.400229	18.334797	-0.051663	2.144256
257.464907	1385.451284	18.339802	-0.051671	2.139038
257.278167	1377.535149	18.344807	-0.051632	2.133805
257.285579	1369.575493	18.349811	-0.051629	2.128549
257.208457	1361.643154	18.354816	-0.051611	2.123290
257.355581	1353.714416	18.359821	-0.051634	2.118041
257.245028	1345.738100	18.364826	-0.051609	2.112723
257.268432	1337.767491	18.369831	-0.051609	2.107408
257.045309	1329.849795	18.374835	-0.051563	2.102092
256.819223	1321.955027	18.379840	-0.051517	2.096777
257.050353	1313.984686	18.384845	-0.051555	2.091442
256.798968	1306.072835	18.389850	-0.051504	2.086086
256.700835	1298.162885	18.394855	-0.051482	2.080732
256.468377	1290.262516	18.399859	-0.051434	2.075357
256.491806	1282.284873	18.404864	-0.051434	2.069942
256.503567	1274.347623	18.409869	-0.051432	2.064538
256.209494	1266.461194	18.414874	-0.051373	2.059125
256.306111	1258.508935	18.419879	-0.051387	2.053691
256.514092	1250.535641	18.424883	-0.051421	2.048240
256.190025	1242.655773	18.429888	-0.051357	2.042785
256.139309	1234.746634	18.434893	-0.051343	2.037322
256.196935	1226.774066	18.439898	-0.051349	2.031812
256.111592	1218.847926	18.444903	-0.051329	2.026305
256.032839	1210.925148	18.449907	-0.051310	2.020786
256.128088	1202.982267	18.454912	-0.051323	2.015255
256.071135	1195.065984	18.459917	-0.051309	2.009712
255.734113	1187.175017	18.464922	-0.051241	2.004142
255.782429	1179.249991	18.469927	-0.051246	1.998573
255.831111	1171.303175	18.474931	-0.051251	1.992973
255.460837	1163.406290	18.479936	-0.051178	1.987349
255.562512	1155.476081	18.484941	-0.051192	1.981735
255.640866	1147.532047	18.489946	-0.051203	1.976092
255.589129	1139.615158	18.494951	-0.051189	1.970439
255.356032	1131.717591	18.499955	-0.051141	1.964764
255.438648	1123.798600	18.504960	-0.051152	1.959091
255.592052	1115.849392	18.509965	-0.051176	1.953387
255.199897	1107.931841	18.514970	-0.051099	1.947631
255.126890	1100.013969	18.519975	-0.051081	1.941892
255.114891	1092.098551	18.524979	-0.051075	1.936144
255.002265	1084.182804	18.529984	-0.051049	1.930368
254.935989	1076.273153	18.534989	-0.051033	1.924584
255.003430	1068.348397	18.539994	-0.051041	1.918786
254.986345	1060.441607	18.544999	-0.051033	1.912975
254.691442	1052.537626	18.550003	-0.050974	1.907116
254.627403	1044.625068	18.555008	-0.050958	1.901260
254.812014	1036.704657	18.560013	-0.050988	1.895407
254.564913	1028.803683	18.565018	-0.050938	1.889502
254.494356	1020.904287	18.570023	-0.050920	1.883599
254.607324	1012.988614	18.575027	-0.050937	1.877687
254.438079	1005.074346	18.580032	-0.050901	1.871725
254.309375	997.178799	18.585037	-0.050873	1.865762
254.215246	989.270492	18.590042	-0.050851	1.859775
254.168941	981.380786	18.595047	-0.050838	1.853788
254.002909	973.476725	18.600051	-0.050803	1.847757
253.950117	965.569361	18.605056	-0.050789	1.841716
254.115168	957.660792	18.610061	-0.050815	1.835680
253.991904	949.753004	18.615066	-0.050788	1.829591
253.875841	941.868678	18.620071	-0.050762	1.823501
253.876739	933.973577	18.625075	-0.050758	1.817396
253.684144	926.083816	18.630080	-0.050718	1.811251
253.537889	918.195384	18.635085	-0.050687	1.805092
253.350004	910.329432	18.640090	-0.050647	1.798924
253.575945	902.374789	18.645095	-0.050685	1.792715
253.444245	894.459346	18.650099	-0.050656	1.786473
253.111746	886.600856	18.655104	-0.050590	1.780228
253.306773	878.691115	18.660109	-0.050622	1.773986
253.281443	870.781944	18.665114	-0.050613	1.767696
253.139136	862.925774	18.670119	-0.050582	1.761410
253.261220	855.025135	18.675123	-0.050601	1.755099
253.032841	847.149342	18.680128	-0.050554	1.748742
252.982958	839.271914	18.685133	-0.050540	1.742382
252.873515	831.404659	18.690138	-0.050516	1.736000
252.905477	823.504322	18.695143	-0.050517	1.729586
252.878159	815.631625	18.700147	-0.050508	1.723162
252.641306	807.789219	18.705152	-0.050460	1.716712
252.797091	799.871043	18.710157	-0.050484	1.710227
252.636892	791.999434	18.715162	-0.050450	1.703714
252.335697	784.164087	18.720167	-0.050390	1.697187
252.517159	776.245192	18.725171	-0.050419	1.690630
252.295817	768.394724	18.730176	-0.050374	1.684050
252.301990	760.541854	18.735181	-0.050371	1.677473
251.995682	752.685526	18.740186	-0.050310	1.670826
251.985383	744.808184	18.745191	-0.050303	1.664174
251.980633	736.940086	18.750195	-0.050298	1.657503
251.780167	729.083312	18.755200	-0.050257	1.650789
251.943120	721.198010	18.760205	-0.050283	1.644073
251.975774	713.339156	18.765210	-0.050285	1.637333
251.899613	705.446955	18.770215	-0.050266	1.630523
251.823127	697.572488	18.775219	-0.050248	1.623699
251.472073	689.768450	18.780224	-0.050178	1.616869
251.551957	681.888817	18.785229	-0.050189	1.610004
251.463406	674.040686	18.790234	-0.050168	1.603114
251.477219	666.198366	18.795239	-0.050166	1.596214
251.393529	658.346346	18.800243	-0.050146	1.589261
251.267594	650.505678	18.805248	-0.050119	1.582282
251.401670	642.651982	18.810253	-0.050139	1.575297
251.087199	634.844778	18.815258	-0.050077	1.568259
250.932374	627.024418	18.820263	-0.050043	1.561199
251.058087	619.165013	18.825267	-0.050063	1.554114
250.860832	611.319274	18.830272	-0.050022	1.546961
250.795407	603.503090	18.835277	-0.050005	1.539821
250.477815	595.704443	18.840282	-0.049942	1.532626
250.491447	587.846404	18.845287	-0.049940	1.525392
250.463269	580.032504	18.850291	-0.049931	1.518159
250.466880	572.177912	18.855296	-0.049927	1.510857
250.321836	564.377599	18.860301	-0.049896	1.503549
250.373387	556.539062	18.865306	-0.049901	1.496198
250.171079	548.744734	18.870311	-0.049859	1.488814
250.088405	540.939249	18.875315	-0.049840	1.481401
249.975503	533.139709	18.880320	-0.049814	1.473952
250.039750	525.266845	18.885325	-0.049822	1.466422
249.820152	517.486993	18.890330	-0.049777	1.458899
249.828691	509.676776	18.895335	-0.049774	1.451343
249.825266	501.871466	18.900339	-0.049770	1.443750
249.524143	494.113180	18.905344	-0.049709	1.436116
249.566870	486.302941	18.910349	-0.049713	1.428445
249.582825	478.492442	18.915354	-0.049712	1.420728
249.404960	470.742817	18.920359	-0.049674	1.412997
249.361594	462.949258	18.925363	-0.049662	1.405203
249.429470	455.154718	18.930368	-0.049671	1.397382
249.300424	447.379278	18.935373	-0.049642	1.389504
249.135871	439.613898	18.940378	-0.049608	1.381585
249.218831	431.828509	18.945383	-0.049619	1.373641
249.446321	424.014941	18.950387	-0.049657	1.365648
249.194892	416.302721	18.955392	-0.049606	1.357630
248.950021	408.572931	18.960397	-0.049556	1.349546
248.880455	400.802359	18.965402	-0.049539	1.341402
248.572669	393.106202	18.970407	-0.049477	1.333245
248.561615	385.339804	18.975411	-0.049471	1.325016
248.495908	377.604401	18.980416	-0.049455	1.316758
248.581823	369.730798	18.985421	-0.049467	1.308327
248.208099	362.033934	18.990426	-0.049393	1.299949
248.047270	354.327275	18.995431	-0.049359	1.291545
248.029535	346.598387	19.000435	-0.049351	1.283087
247.887528	338.896111	19.005440	-0.049321	1.274580
247.920477	331.162715	19.010445	-0.049323	1.266014
247.805387	323.471863	19.015450	-0.049297	1.257410
247.691522	315.775503	19.020455	-0.049272	1.248739
247.808508	308.066616	19.025459	-0.049289	1.240039
247.442803	300.413621	19.030464	-0.049217	1.231247
247.418204	292.715096	19.035469	-0.049208	1.222406
247.345420	285.032926	19.040474	-0.049191	1.213510
246.951982	277.407035	19.045479	-0.049113	1.204551
247.169236	269.703461	19.050483	-0.049150	1.195555
246.935182	262.049558	19.055488	-0.049102	1.186459
246.769945	254.427170	19.060493	-0.049067	1.177344
246.634698	246.776761	19.065498	-0.049038	1.168130
246.752035	239.109658	19.070503	-0.049055	1.158875
246.661855	231.457756	19.075507	-0.049034	1.149521
246.441081	223.841813	19.080512	-0.048989	1.140106
246.474797	216.211341	19.085517	-0.048991	1.130650
246.203791	208.628028	19.090522	-0.048937	1.121107
246.040530	201.047350	19.095527	-0.048902	1.111509
246.105505	193.422958	19.100531	-0.048910	1.101821
245.924836	185.860595	19.105536	-0.048873	1.092074
245.890269	178.285400	19.110541	-0.048862	1.082254
245.806121	170.721285	19.115546	-0.048842	1.072347
245.569071	163.182189	19.120551	-0.048794	1.062347
245.353214	155.665921	19.125555	-0.048750	1.052286
245.222035	148.133359	19.130560	-0.048722	1.042127
245.166014	140.609644	19.135565	-0.048707	1.031897
244.765118	133.138362	19.140570	-0.048628	1.021554
244.602334	125.653461	19.145575	-0.048594	1.011144
244.648730	118.142594	19.150579	-0.048599	1.000640
244.129914	110.716601	19.155584	-0.048498	0.990006
243.815575	103.268390	19.160589	-0.048436	0.979275
243.520779	95.835535	19.165594	-0.048377	0.968452
243.442224	88.395290	19.170599	-0.048358	0.957551
242.867378	81.041535	19.175603	-0.048247	0.946525
242.424287	73.679780	19.180608	-0.048161	0.935391
242.122480	66.311195	19.185613	-0.048101	0.924149
241.655066	59.221813	19.190618	-0.048010	0.913155