Fri Mar 12 11:04:30 2021


Number of Points = 3620

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.545004	0.117733	0.000000	0.000047	0.724197
0.748293	0.113565	0.005005	0.000008	0.724260
0.854758	-0.028672	0.010010	-0.000011	0.724019
0.757918	-0.048227	0.015014	0.000006	0.723947
0.964321	-0.082126	0.020019	-0.000032	0.723953
0.706824	-0.038773	0.025024	0.000016	0.723949
0.611710	-0.019987	0.030029	0.000033	0.723953
0.740050	-0.041422	0.035034	0.000009	0.723956
0.655446	-0.030484	0.040038	0.000025	0.723948
0.652043	-0.024360	0.045043	0.000025	0.723959
0.585020	-0.017867	0.050048	0.000037	0.723949
0.709251	-0.038451	0.055053	0.000014	0.723952
0.666971	-0.029908	0.060058	0.000022	0.723954
0.418455	0.009655	0.065062	0.000068	0.723946
0.791464	-0.052672	0.070067	-0.000002	0.723954
0.573615	-0.018528	0.075072	0.000038	0.723945
0.500867	-0.051929	0.080077	0.000052	0.723855
0.756748	-0.211062	0.085082	0.000004	0.723633
0.734671	-0.210099	0.090086	0.000008	0.723627
0.835779	-0.223303	0.095091	-0.000011	0.723637
0.756011	-0.214099	0.100096	0.000004	0.723627
0.832536	-0.224718	0.105101	-0.000011	0.723634
0.831007	-0.226139	0.110106	-0.000011	0.723631
0.520182	-0.322636	0.115110	0.000047	0.723333
0.683755	-0.348397	0.120115	0.000016	0.723340
0.759133	-0.365421	0.125120	0.000002	0.723334
0.806161	-0.371864	0.130125	-0.000007	0.723338
0.709428	-0.357727	0.135130	0.000011	0.723332
0.548693	-0.499864	0.140134	0.000041	0.722998
0.815142	-0.543944	0.145139	-0.000009	0.723005
0.802232	-0.543217	0.150144	-0.000007	0.723002
0.852212	-0.549193	0.155149	-0.000016	0.723008
0.855572	-0.690084	0.160154	-0.000017	0.722733
0.604325	-0.668478	0.165158	0.000030	0.722688
0.762921	-0.691766	0.170163	0.000000	0.722698
0.755949	-0.730475	0.175168	0.000001	0.722620
0.575699	-0.826552	0.180173	0.000035	0.722369
0.548787	-0.820469	0.185178	0.000039	0.722372
0.442309	-0.804591	0.190182	0.000059	0.722366
0.500470	-0.926104	0.195187	0.000048	0.722148
0.413612	-0.948611	0.200192	0.000064	0.722074
0.563626	-0.975105	0.205197	0.000036	0.722075
0.465845	-1.049578	0.210202	0.000054	0.721894
0.292801	-1.097638	0.215206	0.000086	0.721740
0.424832	-1.116125	0.220211	0.000061	0.721750
0.442214	-1.208204	0.225216	0.000058	0.721576
0.454503	-1.281250	0.230221	0.000056	0.721437
0.462234	-1.279471	0.235226	0.000054	0.721443
0.501542	-1.414712	0.240230	0.000047	0.721191
0.581774	-1.461842	0.245235	0.000031	0.721127
0.288507	-1.432578	0.250240	0.000086	0.721082
0.421102	-1.561793	0.255245	0.000061	0.720875
0.481652	-1.569225	0.260250	0.000050	0.720882
0.473320	-1.684659	0.265254	0.000051	0.720652
0.375839	-1.723316	0.270259	0.000069	0.720542
0.193768	-1.734213	0.275264	0.000103	0.720457
0.122868	-1.840932	0.280269	0.000116	0.720223
0.091223	-1.832821	0.285274	0.000122	0.720228
0.063415	-1.977684	0.290278	0.000127	0.719933
0.069840	-1.994935	0.295283	0.000125	0.719902
-0.390591	-2.003395	0.300288	0.000211	0.719724
-0.758545	-2.002442	0.305293	0.000279	0.719597
-0.897859	-1.989335	0.310298	0.000305	0.719574
-1.191587	-2.093943	0.315302	0.000359	0.719265
-1.347423	-2.062094	0.320307	0.000388	0.719274
-1.925852	-2.037305	0.325312	0.000496	0.719120
-3.181483	-1.895528	0.330317	0.000729	0.718959
-2.471484	-2.020694	0.335322	0.000597	0.718962
-2.823431	-2.015951	0.340326	0.000662	0.718848
-3.787251	-1.945368	0.345331	0.000842	0.718649
-3.325038	-2.032536	0.350336	0.000755	0.718639
-3.947051	-1.920866	0.355341	0.000871	0.718642
-4.253506	-1.995160	0.360346	0.000928	0.718387
-4.400208	-1.987869	0.365350	0.000955	0.718351
-4.634868	-1.941985	0.370355	0.000998	0.718359
-4.413184	-2.001294	0.375360	0.000957	0.718320
-5.200252	-2.014620	0.380365	0.001103	0.718017
-5.140482	-2.021179	0.385370	0.001092	0.718026
-5.930902	-1.885712	0.390374	0.001239	0.718016
-5.546390	-1.952363	0.395379	0.001167	0.718020
-5.494016	-2.085909	0.400384	0.001157	0.717775
-6.712997	-1.906844	0.405389	0.001384	0.717700
-6.319095	-1.971971	0.410394	0.001311	0.717710
-6.270482	-1.987010	0.415398	0.001301	0.717698
-6.348864	-1.988393	0.420403	0.001316	0.717668
-7.233137	-1.978371	0.425408	0.001480	0.717377
-7.543934	-1.920744	0.430413	0.001538	0.717381
-7.451076	-1.934780	0.435418	0.001520	0.717387
-7.524908	-1.926309	0.440422	0.001534	0.717378
-7.501806	-1.927998	0.445427	0.001529	0.717383
-7.298710	-2.049999	0.450432	0.001492	0.717214
-7.970791	-1.996403	0.455437	0.001616	0.717083
-8.195459	-1.954670	0.460442	0.001658	0.717087
-8.618107	-1.884893	0.465446	0.001737	0.717076
-8.342939	-1.928366	0.470451	0.001685	0.717088
-7.936552	-2.006023	0.475456	0.001609	0.717078
-8.853269	-2.007085	0.480461	0.001780	0.716753
-9.070036	-1.964631	0.485466	0.001820	0.716761
-9.775551	-1.844305	0.490470	0.001951	0.716751
-9.075353	-1.963925	0.495475	0.001821	0.716761
-8.875152	-2.002763	0.500480	0.001783	0.716755
-9.088342	-1.963667	0.505485	0.001823	0.716758
-9.911453	-1.950260	0.510490	0.001976	0.716494
-10.477488	-1.874918	0.515494	0.002081	0.716444
-9.704923	-2.008972	0.520499	0.001937	0.716452
-9.567231	-2.035492	0.525504	0.001911	0.716448
-10.390416	-1.889668	0.530509	0.002064	0.716447
-10.216631	-1.917808	0.535514	0.002032	0.716453
-9.861625	-2.038497	0.540518	0.001965	0.716339
-10.589302	-2.009541	0.545523	0.002101	0.716140
-10.452510	-2.037122	0.550528	0.002075	0.716134
-11.298622	-1.888668	0.555533	0.002232	0.716130
-11.740026	-1.806475	0.560538	0.002314	0.716138
-11.060680	-1.932162	0.565542	0.002188	0.716129
-10.479738	-2.032046	0.570547	0.002079	0.716136
-11.345496	-1.984172	0.575552	0.002240	0.715926
-12.394934	-1.819463	0.580557	0.002435	0.715882
-11.721772	-1.936842	0.585562	0.002310	0.715888
-11.283444	-2.018571	0.590566	0.002228	0.715881
-11.560019	-1.963968	0.595571	0.002279	0.715892
-12.083656	-1.873349	0.600576	0.002377	0.715887
-12.150454	-1.864820	0.605581	0.002389	0.715880
-12.392711	-1.985571	0.610586	0.002434	0.715556
-12.433610	-1.984252	0.615590	0.002441	0.715544
-12.627293	-1.946543	0.620595	0.002477	0.715551
-12.939878	-1.893833	0.625600	0.002535	0.715546
-13.254821	-1.837239	0.630605	0.002594	0.715547
-12.807609	-1.914410	0.635610	0.002510	0.715552
-12.243736	-2.041926	0.640614	0.002405	0.715499
-13.509836	-1.948755	0.645619	0.002641	0.715237
-13.838682	-1.893618	0.650624	0.002702	0.715230
-13.829514	-1.895392	0.655629	0.002700	0.715230
-13.036729	-2.033696	0.660634	0.002552	0.715236
-13.202612	-2.009321	0.665638	0.002583	0.715227
-13.588566	-1.936731	0.670643	0.002654	0.715234
-13.920442	-1.943022	0.675648	0.002716	0.715105
-14.898430	-1.869199	0.680653	0.002898	0.714906
-13.872035	-2.049283	0.685658	0.002707	0.714912
-14.389054	-1.962153	0.690662	0.002803	0.714903
-14.983712	-1.851872	0.695667	0.002913	0.714912
-14.832001	-1.881124	0.700672	0.002885	0.714907
-14.456123	-1.951059	0.705677	0.002815	0.714902
-14.429276	-1.975765	0.710682	0.002809	0.714863
-15.477665	-1.920931	0.715686	0.003004	0.714601
-15.218798	-1.961804	0.720691	0.002956	0.714612
-15.569069	-1.902569	0.725696	0.003021	0.714606
-15.602850	-1.898107	0.730701	0.003027	0.714603
-15.440884	-1.924115	0.735706	0.002997	0.714609
-15.122078	-1.984787	0.740710	0.002937	0.714602
-15.369953	-1.948826	0.745715	0.002983	0.714586
-16.295608	-1.940163	0.750720	0.003155	0.714276
-16.399325	-1.920765	0.755725	0.003174	0.714278
-16.298326	-1.937328	0.760730	0.003156	0.714281
-16.403611	-1.923662	0.765734	0.003175	0.714272
-16.367286	-1.927170	0.770739	0.003168	0.714278
-16.540643	-1.896858	0.775744	0.003200	0.714277
-16.488415	-1.908111	0.780749	0.003190	0.714274
-16.275067	-2.036310	0.785754	0.003150	0.714095
-17.432222	-1.897064	0.790758	0.003365	0.713962
-17.584164	-1.864282	0.795763	0.003394	0.713974
-17.360705	-1.907770	0.800768	0.003352	0.713967
-17.319664	-1.916165	0.805773	0.003344	0.713965
-17.101994	-1.950491	0.810778	0.003303	0.713974
-17.651086	-1.857046	0.815782	0.003405	0.713966
-17.424786	-1.922679	0.820787	0.003363	0.713916
-17.679632	-2.011309	0.825792	0.003410	0.713650
-18.023382	-1.950479	0.830797	0.003474	0.713650
-18.379868	-1.882945	0.835802	0.003540	0.713658
-18.167109	-1.925389	0.840806	0.003500	0.713649
-17.875666	-1.973373	0.845811	0.003446	0.713657
-18.264619	-1.906649	0.850816	0.003518	0.713653
-18.208740	-1.968208	0.855821	0.003508	0.713550
-18.859668	-1.943895	0.860826	0.003629	0.713369
-19.067944	-1.911950	0.865830	0.003667	0.713359
-18.925229	-1.933712	0.870835	0.003640	0.713366
-18.884135	-1.941998	0.875840	0.003633	0.713365
-19.023742	-1.921229	0.880845	0.003658	0.713357
-18.917563	-1.934912	0.885850	0.003639	0.713368
-19.138644	-1.956794	0.890854	0.003679	0.713246
-19.907985	-1.929970	0.895859	0.003823	0.713027
-19.691976	-1.969657	0.900864	0.003782	0.713025
-19.923884	-1.929733	0.905869	0.003825	0.713023
-19.854776	-1.937676	0.910874	0.003812	0.713032
-20.283207	-1.867090	0.915878	0.003892	0.713021
-20.232363	-1.872956	0.920883	0.003882	0.713027
-19.767826	-1.974770	0.925888	0.003795	0.712990
-20.937018	-1.908100	0.930893	0.004013	0.712708
-20.826163	-1.924386	0.935898	0.003992	0.712715
-21.086651	-1.882151	0.940902	0.004040	0.712708
-20.691961	-1.949756	0.945907	0.003967	0.712713
-20.962067	-1.903181	0.950912	0.004017	0.712711
-21.198895	-1.863711	0.955917	0.004061	0.712706
-20.730629	-1.943837	0.960922	0.003973	0.712712
-21.062868	-1.997196	0.965926	0.004035	0.712489
-21.781471	-1.920199	0.970931	0.004169	0.712387
-21.610582	-1.950515	0.975936	0.004137	0.712388
-21.823920	-1.913975	0.980941	0.004176	0.712385
-21.789022	-1.917747	0.985946	0.004169	0.712391
-21.525691	-1.969198	0.990950	0.004120	0.712382
-21.627896	-1.948620	0.995955	0.004139	0.712387
-22.175837	-1.959297	1.000960	0.004241	0.712172
-22.699750	-1.907721	1.005965	0.004338	0.712089
-22.243743	-1.986374	1.010970	0.004253	0.712094
-22.940132	-1.865836	1.015974	0.004383	0.712088
-22.840822	-1.880774	1.020979	0.004364	0.712093
-22.507499	-1.941483	1.025984	0.004302	0.712091
-22.513812	-1.942184	1.030989	0.004303	0.712088
-23.003860	-1.950441	1.035994	0.004394	0.711898
-23.974337	-1.848400	1.040998	0.004574	0.711757
-23.208947	-1.980463	1.046003	0.004432	0.711766
-23.591896	-1.913971	1.051008	0.004503	0.711763
-23.920564	-1.856447	1.056013	0.004564	0.711761
-23.475439	-1.932381	1.061018	0.004481	0.711768
-23.814577	-1.875419	1.066022	0.004544	0.711761
-23.638702	-1.915785	1.071027	0.004511	0.711744
-23.820235	-2.027179	1.076032	0.004544	0.711458
-24.374372	-1.931315	1.081037	0.004647	0.711452
-24.860476	-1.840883	1.086042	0.004737	0.711460
-24.325112	-1.939749	1.091046	0.004638	0.711454
-24.117227	-1.974273	1.096051	0.004599	0.711459
-24.697560	-1.872567	1.101056	0.004707	0.711456
-24.733274	-1.868496	1.106061	0.004713	0.711452
-24.796298	-2.009041	1.111066	0.004725	0.711149
-25.476127	-1.894922	1.116070	0.004851	0.711136
-26.070375	-1.787252	1.121075	0.004961	0.711140
-25.169313	-1.945771	1.126080	0.004794	0.711144
-25.165171	-1.948879	1.131085	0.004793	0.711140
-25.391928	-1.907165	1.136090	0.004835	0.711143
-25.444149	-1.903359	1.141094	0.004844	0.711132
-25.395925	-2.006574	1.146099	0.004835	0.710943
-26.431457	-1.858036	1.151104	0.005028	0.710872
-26.494400	-1.846961	1.156109	0.005039	0.710872
-25.870980	-1.955107	1.161114	0.004923	0.710878
-26.353513	-1.873482	1.166118	0.005013	0.710870
-26.433323	-1.856312	1.171123	0.005027	0.710876
-25.982611	-1.936028	1.176128	0.004943	0.710878
-26.332276	-2.004887	1.181133	0.005008	0.710616
-27.417642	-1.849596	1.186138	0.005210	0.710540
-27.414094	-1.853026	1.191142	0.005209	0.710535
-26.847139	-1.952638	1.196147	0.005103	0.710538
-27.033797	-1.920063	1.201152	0.005138	0.710537
-27.390078	-1.859721	1.206157	0.005204	0.710531
-26.728445	-1.972455	1.211162	0.005081	0.710542
-27.206905	-2.007514	1.216166	0.005170	0.710302
-28.204349	-1.869978	1.221171	0.005355	0.710222
-27.777447	-1.945299	1.226176	0.005275	0.710224
-28.063548	-1.899415	1.231181	0.005328	0.710214
-28.283235	-1.856577	1.236186	0.005369	0.710222
-28.183929	-1.879688	1.241190	0.005351	0.710211
-27.644143	-1.970556	1.246195	0.005250	0.710222
-28.023420	-2.018508	1.251200	0.005320	0.709992
-29.216735	-1.856975	1.256205	0.005542	0.709890
-28.592702	-1.963681	1.261210	0.005426	0.709899
-28.729750	-1.943185	1.266214	0.005451	0.709892
-29.136096	-1.868489	1.271219	0.005527	0.709897
-28.988805	-1.894645	1.276224	0.005499	0.709897
-28.901011	-1.912775	1.281229	0.005483	0.709893
-28.955514	-1.996262	1.286234	0.005493	0.709707
-29.962941	-1.875129	1.291238	0.005680	0.709590
-29.630357	-1.930484	1.296243	0.005618	0.709598
-29.551236	-1.943868	1.301248	0.005603	0.709600
-30.065169	-1.855226	1.306253	0.005698	0.709595
-29.561884	-1.940535	1.311258	0.005604	0.709604
-29.547858	-1.947273	1.316262	0.005602	0.709596
-30.119663	-1.966576	1.321267	0.005708	0.709354
-30.778711	-1.892168	1.326272	0.005830	0.709268
-30.306157	-1.980078	1.331277	0.005742	0.709261
-30.596269	-1.922859	1.336282	0.005796	0.709272
-31.112931	-1.836809	1.341286	0.005892	0.709261
-30.808483	-1.888947	1.346291	0.005835	0.709265
-30.235797	-1.990451	1.351296	0.005729	0.709267
-30.944073	-1.967240	1.356301	0.005860	0.709061
-31.678371	-1.884936	1.361306	0.005997	0.708964
-31.351117	-1.949328	1.366310	0.005936	0.708952
-31.500964	-1.919916	1.371315	0.005963	0.708958
-31.775932	-1.869881	1.376320	0.006014	0.708960
-31.594584	-1.904994	1.381325	0.005980	0.708955
-30.905995	-2.024584	1.386330	0.005852	0.708962
-31.652704	-1.997554	1.391334	0.005991	0.708750
-32.610424	-1.880977	1.396339	0.006169	0.708642
-32.157481	-1.961807	1.401344	0.006084	0.708642
-32.381889	-1.923978	1.406349	0.006126	0.708638
-32.469769	-1.904521	1.411354	0.006142	0.708646
-32.120564	-1.969706	1.416358	0.006077	0.708640
-32.523706	-1.897411	1.421363	0.006152	0.708642
-32.807351	-1.937509	1.426368	0.006204	0.708460
-33.397810	-1.887999	1.431373	0.006314	0.708349
-32.814917	-1.986812	1.436378	0.006206	0.708360
-33.533097	-1.865065	1.441382	0.006339	0.708347
-33.583198	-1.854991	1.446387	0.006348	0.708350
-32.815619	-1.990538	1.451392	0.006205	0.708353
-33.269014	-1.913258	1.456397	0.006289	0.708346
-33.618204	-1.954132	1.461402	0.006354	0.708140
-34.397505	-1.880007	1.466406	0.006499	0.708010
-34.088211	-1.934731	1.471411	0.006441	0.708012
-34.261716	-1.904297	1.476416	0.006473	0.708011
-34.387782	-1.884927	1.481421	0.006497	0.708005
-33.902898	-1.966393	1.486426	0.006406	0.708015
-34.188972	-1.919866	1.491430	0.006459	0.708007
-34.281894	-1.964329	1.496435	0.006476	0.707885
-35.149544	-1.901865	1.501440	0.006638	0.707700
-35.045296	-1.924245	1.506445	0.006618	0.707693
-35.287815	-1.877462	1.511450	0.006663	0.707701
-34.961173	-1.939093	1.516454	0.006602	0.707694
-34.821577	-1.962521	1.521459	0.006576	0.707697
-35.400750	-1.857250	1.526464	0.006684	0.707702
-35.472431	-1.852086	1.531469	0.006697	0.707687
-35.308341	-2.034915	1.536474	0.006666	0.707379
-36.028053	-1.908832	1.541478	0.006800	0.707375
-36.389252	-1.841947	1.546483	0.006867	0.707381
-35.646955	-1.974399	1.551488	0.006729	0.707381
-36.072325	-1.904398	1.556493	0.006807	0.707369
-36.196632	-1.878026	1.561498	0.006830	0.707378
-35.982556	-1.920254	1.566502	0.006790	0.707370
-36.384170	-1.988219	1.571507	0.006865	0.707091
-36.790819	-1.920658	1.576512	0.006941	0.707081
-37.144038	-1.860248	1.581517	0.007006	0.707076
-36.733488	-1.930576	1.586522	0.006929	0.707082
-36.819275	-1.918614	1.591526	0.006945	0.707076
-37.156695	-1.856783	1.596531	0.007008	0.707080
-36.595760	-1.955433	1.601536	0.006903	0.707083
-37.463654	-1.956933	1.606541	0.007065	0.706770
-38.118946	-1.847183	1.611546	0.007186	0.706756
-37.871989	-1.896514	1.616550	0.007140	0.706745
-37.663476	-1.931763	1.621555	0.007101	0.706750
-37.847640	-1.897794	1.626560	0.007135	0.706752
-38.237608	-1.831026	1.631565	0.007208	0.706747
-37.668651	-1.929205	1.636570	0.007102	0.706754
-37.943051	-1.944079	1.641574	0.007153	0.706626
-38.947091	-1.858632	1.646579	0.007339	0.706439
-38.235640	-1.984118	1.651584	0.007207	0.706442
-38.757485	-1.894733	1.656589	0.007304	0.706435
-38.791460	-1.884196	1.661594	0.007310	0.706444
-38.663461	-1.910999	1.666598	0.007286	0.706437
-38.573330	-1.926003	1.671603	0.007269	0.706439
-38.502250	-2.011868	1.676608	0.007256	0.706292
-39.697976	-1.885446	1.681613	0.007478	0.706118
-39.101023	-1.986254	1.686618	0.007367	0.706130
-39.674263	-1.888325	1.691622	0.007473	0.706122
-39.760890	-1.871121	1.696627	0.007489	0.706126
-39.151748	-1.978723	1.701632	0.007375	0.706128
-39.535821	-1.913932	1.706637	0.007447	0.706121
-39.674035	-1.973748	1.711642	0.007472	0.705952
-40.494783	-1.874929	1.716646	0.007625	0.705856
-40.468446	-1.878640	1.721651	0.007620	0.705859
-40.615381	-1.851346	1.726656	0.007647	0.705861
-40.671944	-1.844897	1.731661	0.007657	0.705854
-40.265901	-1.913230	1.736666	0.007582	0.705863
-40.298812	-1.910143	1.741670	0.007588	0.705858
-40.685505	-1.915388	1.746675	0.007659	0.705709
-41.252847	-1.906255	1.751680	0.007765	0.705524
-40.880043	-1.974756	1.756685	0.007695	0.705520
-41.520775	-1.856525	1.761690	0.007814	0.705529
-41.775121	-1.815901	1.766694	0.007861	0.705520
-41.246246	-1.908617	1.771699	0.007763	0.705523
-41.200569	-1.914729	1.776704	0.007754	0.705528
-41.610471	-1.893655	1.781709	0.007830	0.705423
-42.288738	-1.876686	1.786714	0.007956	0.705214
-42.298275	-1.878927	1.791718	0.007958	0.705207
-42.759597	-1.797176	1.796723	0.008044	0.705206
-42.276464	-1.881004	1.801728	0.007953	0.705211
-42.042939	-1.928979	1.806733	0.007910	0.705199
-42.530292	-1.836114	1.811738	0.008000	0.705211
-42.146158	-1.906170	1.816742	0.007929	0.705208
-42.500263	-1.981799	1.821747	0.007994	0.704929
-43.483542	-1.825208	1.826752	0.008177	0.704892
-43.649241	-1.800925	1.831757	0.008208	0.704882
-42.851276	-1.939720	1.836762	0.008059	0.704889
-43.065104	-1.906352	1.841766	0.008099	0.704880
-43.336100	-1.857833	1.846771	0.008149	0.704881
-43.213636	-1.876203	1.851776	0.008126	0.704888
-43.172851	-1.973082	1.856781	0.008118	0.704708
-44.156826	-1.856218	1.861786	0.008301	0.704590
-44.109136	-1.868503	1.866790	0.008292	0.704583
-43.977282	-1.892655	1.871795	0.008268	0.704582
-43.856505	-1.911578	1.876800	0.008245	0.704588
-44.168466	-1.859318	1.881805	0.008303	0.704581
-43.782734	-1.923579	1.886810	0.008231	0.704591
-43.943880	-2.015630	1.891814	0.008261	0.704348
-45.005108	-1.871253	1.896819	0.008458	0.704258
-44.753675	-1.915950	1.901824	0.008411	0.704258
-44.853960	-1.902974	1.906829	0.008429	0.704249
-45.020179	-1.868719	1.911834	0.008460	0.704259
-45.035028	-1.869737	1.916838	0.008463	0.704252
-44.708992	-1.925604	1.921843	0.008402	0.704256
-45.014094	-2.002069	1.926848	0.008459	0.703993
-46.147529	-1.823546	1.931853	0.008669	0.703946
-45.778350	-1.886373	1.936858	0.008600	0.703952
-45.460270	-1.946591	1.941862	0.008541	0.703945
-46.035231	-1.846043	1.946867	0.008648	0.703942
-45.964562	-1.854604	1.951872	0.008635	0.703950
-45.761559	-1.893106	1.956877	0.008597	0.703946
-45.769725	-2.004267	1.961882	0.008598	0.703719
-46.831931	-1.859473	1.966886	0.008795	0.703630
-46.760740	-1.872114	1.971891	0.008782	0.703630
-46.368690	-1.939253	1.976896	0.008709	0.703636
-46.911676	-1.848232	1.981901	0.008810	0.703625
-46.527299	-1.911838	1.986906	0.008738	0.703635
-46.276797	-1.959929	1.991910	0.008691	0.703629
-47.120679	-1.943379	1.996915	0.008848	0.703359
-47.476712	-1.890860	2.001920	0.008914	0.703337
-47.405658	-1.902843	2.011917	0.008901	0.703339
-47.335171	-1.915847	2.021914	0.008887	0.703339
-47.472776	-1.892989	2.031910	0.008912	0.703336
-47.232458	-1.936777	2.041907	0.008867	0.703335
-47.474689	-1.893251	2.051904	0.008912	0.703336
-47.184400	-1.992904	2.061901	0.008858	0.703240
-47.771773	-1.860667	2.071898	0.008967	0.703297
-47.395423	-1.908967	2.081894	0.008896	0.703335
-47.250992	-1.934149	2.091891	0.008869	0.703337
-47.556889	-1.880743	2.101888	0.008925	0.703336
-47.759245	-1.843746	2.111885	0.008963	0.703338
-47.369540	-1.913704	2.121882	0.008890	0.703338
-47.644593	-1.866378	2.131878	0.008941	0.703335
-47.265028	-1.869563	2.141875	0.008870	0.703466
-46.732813	-1.883686	2.151872	0.008770	0.703630
-46.700924	-1.889808	2.161869	0.008764	0.703630
-46.887810	-1.856538	2.171866	0.008798	0.703630
-46.871288	-1.833003	2.181862	0.008795	0.703685
-45.922890	-1.872869	2.191859	0.008618	0.703946
-45.925150	-1.872089	2.201856	0.008618	0.703947
-45.867921	-1.882923	2.211853	0.008607	0.703947
-45.739247	-1.864646	2.221850	0.008582	0.704031
-45.108811	-1.865430	2.231846	0.008465	0.704257
-44.930345	-1.897839	2.241843	0.008431	0.704256
-45.184969	-1.851098	2.251840	0.008478	0.704259
-44.732472	-1.855212	2.261837	0.008393	0.704415
-44.215085	-1.860830	2.271834	0.008297	0.704590
-44.273580	-1.851498	2.281830	0.008307	0.704588
-44.045657	-1.894237	2.291827	0.008264	0.704585
-43.510014	-1.858160	2.301824	0.008164	0.704851
-43.028704	-1.927214	2.311821	0.008074	0.704885
-43.013810	-1.929608	2.321818	0.008071	0.704886
-43.209384	-1.891843	2.331814	0.008107	0.704893
-42.532496	-1.857709	2.341811	0.007981	0.705205
-42.501470	-1.864648	2.351808	0.007975	0.705203
-42.218726	-1.913704	2.361805	0.007922	0.705207
-42.085589	-1.845744	2.371802	0.007896	0.705392
-41.520006	-1.883669	2.381798	0.007791	0.705519
-41.530427	-1.882132	2.391795	0.007792	0.705519
-41.493106	-1.885106	2.401792	0.007785	0.705527
-40.495550	-1.898619	2.411789	0.007599	0.705859
-40.523202	-1.893194	2.421786	0.007604	0.705860
-40.662848	-1.869748	2.431782	0.007629	0.705858
-40.314762	-1.885760	2.441779	0.007564	0.705952
-39.811632	-1.890416	2.451776	0.007470	0.706123
-39.754456	-1.900346	2.461773	0.007459	0.706125
-39.924677	-1.870789	2.471770	0.007490	0.706124
-38.896992	-1.905505	2.481766	0.007299	0.706423
-39.113743	-1.859022	2.491763	0.007339	0.706439
-38.980169	-1.881908	2.501760	0.007313	0.706442
-38.501345	-1.886173	2.511757	0.007224	0.706606
-38.269067	-1.856080	2.521754	0.007180	0.706750
-38.153057	-1.877547	2.531750	0.007158	0.706749
-38.210633	-1.832079	2.541747	0.007169	0.706820
-37.245620	-1.876795	2.551744	0.006989	0.707077
-37.060259	-1.908754	2.561741	0.006954	0.707080
-37.403813	-1.845969	2.571738	0.007017	0.707084
-36.504154	-1.885875	2.581734	0.006849	0.707326
-36.636346	-1.839345	2.591731	0.006874	0.707373
-36.360040	-1.887124	2.601728	0.006822	0.707377
-36.151465	-1.858059	2.611725	0.006783	0.707510
-35.583449	-1.865189	2.621722	0.006676	0.707700
-35.537968	-1.872487	2.631718	0.006668	0.707702
-35.806835	-1.812766	2.641715	0.006717	0.707726
-34.684462	-1.870964	2.651712	0.006508	0.708012
-34.521866	-1.898549	2.661709	0.006477	0.708015
-34.689593	-1.869716	2.671706	0.006508	0.708014
-34.039323	-1.884726	2.681702	0.006387	0.708217
-33.782894	-1.865002	2.691699	0.006339	0.708348
-33.645950	-1.890627	2.701696	0.006313	0.708347
-33.435327	-1.927747	2.711693	0.006273	0.708348
-33.225679	-1.849190	2.721690	0.006234	0.708581
-32.534803	-1.945178	2.731686	0.006105	0.708636
-32.980229	-1.867242	2.741683	0.006187	0.708634
-32.465242	-1.926377	2.751680	0.006091	0.708700
-31.978815	-1.885299	2.761677	0.006000	0.708957
-31.667918	-1.941029	2.771674	0.005942	0.708957
-32.034674	-1.876180	2.781670	0.006010	0.708957
-31.419233	-1.888231	2.791667	0.005895	0.709153
-30.981822	-1.914024	2.801664	0.005813	0.709258
-31.104619	-1.889452	2.811661	0.005835	0.709264
-31.093771	-1.863664	2.821658	0.005833	0.709320
-30.146450	-1.894916	2.831654	0.005656	0.709596
-30.391145	-1.851862	2.841651	0.005701	0.709596
-30.128998	-1.897651	2.851648	0.005652	0.709598
-29.831839	-1.838225	2.861645	0.005596	0.709824
-29.311184	-1.895099	2.871642	0.005499	0.709896
-29.480374	-1.867222	2.881638	0.005530	0.709892
-29.224652	-1.847750	2.891635	0.005482	0.710023
-28.313925	-1.914296	2.901632	0.005312	0.710215
-28.748966	-1.835602	2.911629	0.005393	0.710218
-28.268225	-1.921712	2.921626	0.005303	0.710218
-27.848530	-1.849235	2.931622	0.005225	0.710513
-27.556271	-1.892678	2.941619	0.005170	0.710531
-27.644286	-1.877040	2.951616	0.005186	0.710532
-27.589000	-1.798344	2.961613	0.005175	0.710709
-26.539652	-1.903815	2.971610	0.004979	0.710873
-26.864343	-1.846236	2.981606	0.005039	0.710873
-26.640375	-1.884824	2.991603	0.004997	0.710876
-26.282661	-1.817604	3.001600	0.004930	0.711138
-26.152983	-1.841660	3.011597	0.004906	0.711137
-25.984722	-1.871807	3.021594	0.004874	0.711138
-25.623041	-1.805518	3.031590	0.004806	0.711399
-25.378500	-1.823674	3.041587	0.004760	0.711451
-25.398747	-1.819720	3.051584	0.004764	0.711452
-24.961583	-1.788023	3.061581	0.004682	0.711671
-24.416954	-1.841689	3.071578	0.004580	0.711759
-24.687991	-1.795124	3.081574	0.004630	0.711756
-23.985461	-1.824856	3.091571	0.004499	0.711947
-23.716284	-1.802244	3.101568	0.004449	0.712088
-23.390242	-1.860386	3.111565	0.004388	0.712089
-23.344434	-1.861417	3.121562	0.004379	0.712104
-22.901041	-1.800080	3.131558	0.004296	0.712384
-22.617363	-1.850986	3.141555	0.004243	0.712384
-22.612712	-1.851939	3.151552	0.004241	0.712385
-22.175322	-1.830212	3.161549	0.004160	0.712584
-21.951212	-1.807823	3.171546	0.004117	0.712709
-21.852625	-1.825042	3.181542	0.004099	0.712710
-21.670011	-1.826261	3.191539	0.004064	0.712773
-21.402848	-1.747913	3.201536	0.004014	0.713024
-20.963453	-1.826719	3.211533	0.003932	0.713024
-21.007684	-1.817077	3.221530	0.003940	0.713028
-20.318077	-1.775172	3.231526	0.003811	0.713357
-20.248808	-1.787362	3.241523	0.003798	0.713358
-20.094202	-1.816289	3.251520	0.003769	0.713356
-19.879340	-1.764199	3.261517	0.003728	0.713536
-19.499656	-1.772661	3.271514	0.003657	0.713655
-19.289505	-1.811445	3.281510	0.003618	0.713653
-19.217973	-1.775570	3.291507	0.003604	0.713750
-18.762992	-1.748511	3.301504	0.003519	0.713966
-18.711623	-1.756411	3.311501	0.003509	0.713969
-18.734392	-1.716887	3.321498	0.003513	0.714040
-18.121567	-1.706611	3.331494	0.003398	0.714278
-18.053181	-1.721004	3.341491	0.003385	0.714274
-17.730640	-1.756440	3.351488	0.003325	0.714319
-17.193899	-1.706462	3.361485	0.003224	0.714609
-16.987616	-1.743887	3.371482	0.003186	0.714608
-16.901528	-1.760882	3.381478	0.003169	0.714606
-16.576729	-1.693480	3.391475	0.003108	0.714855
-16.401104	-1.698273	3.401472	0.003075	0.714908
-16.319009	-1.713454	3.411469	0.003060	0.714908
-15.920177	-1.675375	3.421466	0.002985	0.715125
-15.708798	-1.659579	3.431462	0.002945	0.715232
-15.648089	-1.672645	3.441459	0.002934	0.715228
-15.325418	-1.622955	3.451456	0.002873	0.715441
-14.860052	-1.654587	3.461453	0.002786	0.715544
-14.851229	-1.656637	3.471450	0.002784	0.715544
-14.699488	-1.570375	3.481446	0.002755	0.715769
-14.269642	-1.591512	3.491443	0.002675	0.715879
-14.341721	-1.578756	3.501440	0.002688	0.715880
-14.012279	-1.532930	3.511437	0.002626	0.716088
-14.051933	-1.503386	3.521434	0.002633	0.716133
-13.822334	-1.505194	3.531430	0.002590	0.716211
-13.451606	-1.452622	3.541427	0.002521	0.716447
-13.397476	-1.462465	3.551424	0.002510	0.716447
-13.275836	-1.362639	3.561421	0.002487	0.716688
-12.974817	-1.383533	3.571418	0.002431	0.716754
-12.838389	-1.336524	3.581414	0.002405	0.716896
-12.452698	-1.311187	3.591411	0.002333	0.717083
-12.306043	-1.321314	3.601408	0.002305	0.717115
-11.814865	-1.273875	3.611405	0.002213	0.717382
-11.703908	-1.293998	3.621402	0.002192	0.717382
-11.353632	-1.244732	3.631398	0.002126	0.717604
-10.942319	-1.269923	3.641395	0.002050	0.717700
-10.653368	-1.299528	3.651392	0.001995	0.717744
-10.130507	-1.254796	3.661389	0.001898	0.718017
-10.004595	-1.277503	3.671386	0.001874	0.718017
-9.726335	-1.266106	3.681382	0.001822	0.718138
-9.263290	-1.244001	3.691379	0.001735	0.718345
-8.743445	-1.335010	3.701376	0.001638	0.718349
-8.491822	-1.354064	3.711373	0.001591	0.718401
-8.247285	-1.275183	3.721370	0.001545	0.718643
-7.937945	-1.330003	3.731366	0.001487	0.718644
-7.744334	-1.366628	3.741363	0.001450	0.718641
-7.646477	-1.259717	3.751360	0.001432	0.718887
-7.370107	-1.270600	3.761357	0.001380	0.718963
-6.850750	-1.364606	3.771354	0.001283	0.718961
-6.896404	-1.277049	3.781350	0.001291	0.719118
-6.567034	-1.260703	3.791347	0.001229	0.719267
-6.241576	-1.319501	3.801344	0.001168	0.719266
-6.192292	-1.279614	3.811341	0.001159	0.719363
-5.780024	-1.231976	3.821338	0.001082	0.719602
-5.588204	-1.269233	3.831334	0.001045	0.719597
-5.474009	-1.278828	3.841331	0.001024	0.719619
-4.946106	-1.232936	3.851328	0.000925	0.719895
-4.717673	-1.273303	3.861325	0.000882	0.719896
-4.494808	-1.311924	3.871322	0.000840	0.719899
-4.210666	-1.244981	3.881318	0.000787	0.720131
-3.791096	-1.274665	3.891315	0.000709	0.720221
-3.728674	-1.285743	3.901312	0.000697	0.720222
-3.237327	-1.349634	3.911309	0.000605	0.720269
-2.817233	-1.287303	3.921306	0.000526	0.720540
-2.363508	-1.369217	3.931302	0.000441	0.720538
-2.239092	-1.392050	3.941299	0.000418	0.720537
-1.994994	-1.435362	3.951296	0.000372	0.720538
-1.635368	-1.351919	3.961293	0.000305	0.720829
-1.507417	-1.350516	3.971290	0.000280	0.720878
-1.450498	-1.362243	3.981286	0.000269	0.720875
-1.350121	-1.380040	3.991283	0.000250	0.720876
-1.355791	-1.269105	4.001280	0.000251	0.721093
-1.121719	-1.296166	4.011277	0.000207	0.721123
-1.206696	-1.281671	4.021274	0.000222	0.721122
-0.953101	-1.187888	4.031270	0.000175	0.721396
-0.923145	-1.172950	4.041267	0.000169	0.721436
-0.974586	-1.122287	4.051264	0.000178	0.721519
-0.692124	-1.057110	4.061261	0.000125	0.721746
-0.817022	-1.029662	4.071258	0.000148	0.721757
-0.829825	-0.865161	4.081254	0.000150	0.722077
-0.841671	-0.848728	4.091251	0.000152	0.722106
-0.656333	-0.748887	4.101248	0.000117	0.722367
-0.425820	-0.740252	4.111245	0.000073	0.722465
-0.460782	-0.616170	4.121242	0.000079	0.722697
-0.371233	-0.540510	4.131238	0.000062	0.722878
-0.337068	-0.482457	4.141235	0.000056	0.723004
-0.228594	-0.332172	4.151232	0.000035	0.723338
-0.222575	-0.259578	4.161229	0.000033	0.723483
-0.013174	-0.213768	4.171226	-0.000006	0.723646
-0.063400	-0.048440	4.181222	0.000003	0.723954
-0.078234	0.062007	4.191219	0.000005	0.724165
0.000000	0.197502	4.201216	-0.000010	0.724459
0.070945	0.819284	4.206221	-0.000024	0.725700
0.178067	2.069795	4.211226	-0.000045	0.728177
0.670913	3.853813	4.216230	-0.000138	0.731814
0.922811	6.232295	4.221235	-0.000186	0.736495
1.067885	9.141715	4.226240	-0.000216	0.742126
1.454609	12.486147	4.231245	-0.000290	0.748621
2.082751	16.243788	4.236250	-0.000410	0.755915
2.461797	20.451507	4.241254	-0.000483	0.763894
2.815986	25.070070	4.246259	-0.000552	0.772536
3.327176	30.024469	4.251264	-0.000651	0.781742
3.630265	35.359957	4.256269	-0.000711	0.791458
4.328899	40.949183	4.261274	-0.000845	0.801629
4.887413	46.861732	4.266278	-0.000953	0.812194
5.212962	53.104369	4.271283	-0.001018	0.823121
5.581752	59.609584	4.276288	-0.001091	0.834363
6.626651	66.205301	4.281293	-0.001290	0.845808
7.782108	73.041891	4.286298	-0.001510	0.857530
7.938597	80.241353	4.291302	-0.001544	0.869398
8.375643	87.577804	4.296307	-0.001630	0.881406
8.943622	95.070276	4.301312	-0.001741	0.893536
9.428812	102.713286	4.306317	-0.001836	0.905717
11.240055	110.312561	4.311322	-0.002179	0.918027
12.558717	118.091767	4.316326	-0.002430	0.930316
15.498157	125.741022	4.321331	-0.002982	0.942675
16.062496	133.946095	4.326336	-0.003093	0.955081
16.709320	142.189707	4.331341	-0.003219	0.967406
17.571191	150.502277	4.336346	-0.003385	0.979729
18.132969	158.933627	4.341350	-0.003495	0.991993
18.673657	167.404669	4.346355	-0.003601	1.004158
19.574894	175.857392	4.351360	-0.003775	1.016239
20.233079	184.381412	4.356365	-0.003903	1.028218
21.394855	192.875576	4.361370	-0.004125	1.040137
22.124237	201.468083	4.366374	-0.004267	1.051951
22.886061	210.080388	4.371379	-0.004414	1.063668
23.221839	218.798253	4.376384	-0.004483	1.075299
23.987311	227.401574	4.381389	-0.004631	1.086753
24.934207	236.012776	4.386394	-0.004813	1.098137
25.227800	244.729427	4.391398	-0.004874	1.109394
25.789562	253.390145	4.396403	-0.004984	1.120527
26.631408	262.016077	4.401408	-0.005147	1.131566
27.215480	270.668471	4.406413	-0.005261	1.142475
28.090036	279.318160	4.411418	-0.005430	1.153339
28.556976	287.970610	4.416422	-0.005523	1.164020
29.106257	296.608969	4.421427	-0.005631	1.174604
29.758047	305.209716	4.426432	-0.005758	1.185068
30.270541	313.832478	4.431437	-0.005859	1.195439
30.994631	322.400659	4.436442	-0.006000	1.205698
31.413122	331.013991	4.441446	-0.006084	1.215862
31.797240	339.606384	4.446451	-0.006161	1.225911
32.676125	348.135287	4.451456	-0.006330	1.235902
33.318362	356.648260	4.456461	-0.006456	1.245748
34.017512	365.180402	4.461466	-0.006592	1.255549
34.498666	373.703229	4.466470	-0.006687	1.265222
35.005952	382.232843	4.471475	-0.006787	1.274834
35.387129	390.754962	4.476480	-0.006864	1.284342
35.912559	399.234611	4.481485	-0.006967	1.293760
36.593841	407.681914	4.486490	-0.007100	1.303103
36.874073	416.271238	4.491494	-0.007158	1.312460
37.332687	424.736110	4.496499	-0.007249	1.321650
38.509697	433.038445	4.501504	-0.007474	1.330730
39.032937	441.450428	4.506509	-0.007577	1.339749
39.470832	449.871742	4.511514	-0.007664	1.348702
39.866002	458.296672	4.516518	-0.007743	1.357592
40.383395	466.661443	4.521523	-0.007845	1.366383
41.067509	475.036877	4.526528	-0.007978	1.375157
41.409636	483.417201	4.531533	-0.008048	1.383822
42.498876	491.715598	4.536538	-0.008256	1.392476
42.828415	500.094936	4.541542	-0.008323	1.401030
43.160884	508.463306	4.546547	-0.008391	1.409522
43.840837	516.787750	4.551552	-0.008523	1.417976
44.175459	525.128665	4.556557	-0.008591	1.426340
44.606637	533.481990	4.561562	-0.008677	1.434682
45.238549	541.766324	4.566566	-0.008800	1.442941
45.784511	550.068289	4.571571	-0.008907	1.451157
46.004164	558.433496	4.576576	-0.008954	1.459334
46.190712	566.764451	4.581581	-0.008994	1.467428
46.916167	575.073533	4.586586	-0.009135	1.475542
47.803296	583.269173	4.591590	-0.009306	1.483527
48.680524	591.495878	4.596595	-0.009474	1.491498
49.225697	599.784045	4.601600	-0.009582	1.499432
49.727372	608.049069	4.606605	-0.009681	1.507297
50.381797	616.317882	4.611610	-0.009808	1.515146
50.608764	624.612608	4.616614	-0.009856	1.522915
51.008439	632.879627	4.621619	-0.009936	1.530645
51.484470	641.151340	4.626624	-0.010030	1.538351
51.642859	649.431330	4.631629	-0.010065	1.545979
52.164738	657.699768	4.636634	-0.010168	1.553612
52.651169	665.916021	4.641638	-0.010264	1.561156
53.428185	674.090784	4.646643	-0.010414	1.568668
53.870683	682.341282	4.651648	-0.010502	1.576163
54.103484	690.586887	4.656653	-0.010551	1.583589
54.436127	698.854054	4.661658	-0.010619	1.591013
54.985684	707.049828	4.666662	-0.010726	1.598370
55.647457	715.216653	4.671667	-0.010855	1.605683
55.997262	723.474932	4.676672	-0.010926	1.612999
56.326465	731.687305	4.681677	-0.010993	1.620240
56.777206	739.902326	4.686682	-0.011082	1.627467
57.020354	748.195159	4.691686	-0.011133	1.634700
57.224972	756.394011	4.696691	-0.011177	1.641816
57.748576	764.560784	4.701696	-0.011280	1.648917
58.251318	772.735306	4.706701	-0.011379	1.655990
58.751145	780.911924	4.711706	-0.011477	1.663035
59.247581	789.091755	4.716710	-0.011575	1.670053
59.873396	797.262575	4.721715	-0.011697	1.677050
60.040799	805.476789	4.726720	-0.011734	1.683994
60.521859	813.641033	4.731725	-0.011829	1.690909
60.929658	821.849136	4.736730	-0.011911	1.697822
61.475837	829.993785	4.741734	-0.012018	1.704673
61.846160	838.200275	4.746739	-0.012092	1.711524
62.361107	846.377720	4.751744	-0.012194	1.718342
62.703185	854.508122	4.756749	-0.012263	1.725073
63.233046	862.677846	4.761754	-0.012367	1.731833
63.759298	870.823327	4.766758	-0.012471	1.738547
64.398251	878.951469	4.771763	-0.012595	1.745235
64.775053	887.151502	4.776768	-0.012671	1.751923
64.939065	895.350207	4.781773	-0.012707	1.758557
65.233495	903.510489	4.786778	-0.012767	1.765151
65.656093	911.672858	4.791782	-0.012851	1.771739
65.965833	919.849107	4.796787	-0.012914	1.778299
66.437401	927.983902	4.801792	-0.013008	1.784821
66.763785	936.182148	4.806797	-0.013074	1.791353
67.448423	944.322626	4.811802	-0.013207	1.797858
67.784018	952.445451	4.816806	-0.013275	1.804284
67.947303	960.612047	4.821811	-0.013311	1.810700
68.503968	968.739846	4.826816	-0.013420	1.817111
68.666873	976.889865	4.831821	-0.013456	1.823469
69.173069	985.018672	4.836826	-0.013556	1.829829
69.808714	993.124366	4.841830	-0.013679	1.836165
70.211992	1001.252926	4.846835	-0.013760	1.842468
70.699796	1009.398799	4.851840	-0.013856	1.848774
71.127692	1017.537344	4.856845	-0.013942	1.855045
71.684996	1025.656545	4.861850	-0.014051	1.861295
72.220934	1033.781511	4.866854	-0.014156	1.867526
72.610466	1041.960194	4.871859	-0.014234	1.873760
73.561050	1050.010905	4.876864	-0.014417	1.879941
74.421817	1058.075419	4.881869	-0.014582	1.886102
74.799914	1066.253627	4.886874	-0.014658	1.892272
75.339023	1074.378758	4.891878	-0.014764	1.898401
75.751042	1082.509596	4.896883	-0.014846	1.904500
76.069499	1090.676633	4.901888	-0.014911	1.910596
76.383589	1098.822525	4.906893	-0.014975	1.916656
76.815331	1106.936227	4.911898	-0.015061	1.922686
77.061901	1115.089483	4.916902	-0.015112	1.928706
77.311017	1123.234355	4.921907	-0.015164	1.934701
77.699846	1131.349679	4.926912	-0.015242	1.940672
78.006076	1139.467553	4.931917	-0.015305	1.946616
78.172516	1147.664887	4.936922	-0.015341	1.952585
78.644358	1155.756811	4.941926	-0.015434	1.958493
78.790344	1163.858442	4.946931	-0.015467	1.964355
79.147325	1171.975049	4.951936	-0.015539	1.970232
79.544981	1180.057399	4.956941	-0.015619	1.976072
80.013161	1188.145851	4.961946	-0.015711	1.981906
80.717880	1196.204262	4.966950	-0.015848	1.987727
81.314235	1204.307852	4.971955	-0.015964	1.993551
81.682332	1212.422132	4.976960	-0.016038	1.999341
81.942509	1220.524065	4.981965	-0.016092	2.005095
82.100875	1228.679666	4.986970	-0.016127	2.010859
82.744154	1236.752632	4.991974	-0.016252	2.016599
83.545758	1244.790964	4.996979	-0.016407	2.022315
83.883566	1252.940130	5.001984	-0.016476	2.028044
84.363620	1261.071718	5.006989	-0.016570	2.033759
84.942026	1269.157678	5.011994	-0.016684	2.039437
85.169349	1277.271075	5.016998	-0.016731	2.045082
85.228613	1285.411837	5.022003	-0.016748	2.050713
85.758739	1293.513320	5.027008	-0.016852	2.056349
85.875954	1301.629640	5.032013	-0.016879	2.061938
86.148398	1309.729904	5.037018	-0.016936	2.067516
86.216468	1317.878899	5.042022	-0.016954	2.073093
86.649479	1325.934816	5.047027	-0.017040	2.078627
87.010121	1334.030909	5.052032	-0.017112	2.084166
87.234847	1342.119257	5.057037	-0.017160	2.089672
87.557210	1350.235074	5.062042	-0.017225	2.095192
87.934387	1358.292539	5.067046	-0.017301	2.100663
88.442639	1366.341429	5.072051	-0.017401	2.106127
88.901044	1374.488726	5.077056	-0.017492	2.111638
89.216470	1382.597263	5.082061	-0.017556	2.117094
89.260404	1390.708972	5.087066	-0.017570	2.122513
89.681467	1398.767453	5.092070	-0.017654	2.127918
89.964129	1406.859831	5.097075	-0.017712	2.133319
90.179062	1414.956242	5.102080	-0.017757	2.138702
90.429760	1423.021265	5.107085	-0.017809	2.144054
90.926136	1431.096613	5.112090	-0.017907	2.149423
91.111269	1439.213026	5.117094	-0.017947	2.154776
91.490917	1447.262661	5.122099	-0.018023	2.160091
91.921829	1455.342074	5.127104	-0.018109	2.165416
92.159569	1463.434008	5.132109	-0.018159	2.170718
92.340417	1471.560491	5.137114	-0.018198	2.176025
92.420761	1479.655283	5.142118	-0.018218	2.181289
92.682106	1487.726670	5.147123	-0.018272	2.186541
93.016516	1495.843605	5.152128	-0.018340	2.191818
93.309137	1503.914509	5.157133	-0.018400	2.197047
93.786448	1511.954008	5.162138	-0.018494	2.202261
94.082211	1520.020008	5.167142	-0.018555	2.207463
94.485922	1528.082496	5.172147	-0.018635	2.212660
95.360617	1536.106835	5.177152	-0.018804	2.217863
95.828784	1544.167269	5.182157	-0.018896	2.223040
96.190712	1552.266414	5.187162	-0.018969	2.228220
96.291350	1560.422007	5.192166	-0.018993	2.233401
96.637846	1568.484185	5.197171	-0.019063	2.238532
97.275303	1576.524993	5.202176	-0.019187	2.243664
97.457978	1584.619548	5.207181	-0.019227	2.248777
98.058464	1592.693653	5.212186	-0.019344	2.253903
98.313176	1600.787036	5.217190	-0.019397	2.258998
98.522632	1608.866943	5.222195	-0.019442	2.264070
98.860732	1616.962570	5.227200	-0.019510	2.269152
99.096113	1625.135494	5.232205	-0.019559	2.274261
99.203994	1633.195685	5.237210	-0.019585	2.279277
99.189208	1641.269230	5.242214	-0.019588	2.284281
99.491965	1649.299776	5.247219	-0.019649	2.289274
100.013791	1657.356913	5.252224	-0.019752	2.294291
99.972456	1665.442485	5.257229	-0.019750	2.299267
100.354583	1673.481834	5.262234	-0.019826	2.304239
100.939125	1681.524585	5.267238	-0.019941	2.309220
101.310916	1689.592273	5.272243	-0.020015	2.314187
101.474292	1697.680710	5.277248	-0.020051	2.319139
101.833365	1705.725221	5.282253	-0.020123	2.324070
102.193407	1713.802107	5.287258	-0.020196	2.329010
102.441035	1721.890834	5.292262	-0.020247	2.333937
102.705724	1729.948051	5.297267	-0.020302	2.338836
102.992072	1738.033642	5.302272	-0.020361	2.343744
102.979140	1746.129245	5.307277	-0.020364	2.348623
103.545331	1754.194496	5.312282	-0.020475	2.353521
103.852402	1762.250000	5.317286	-0.020538	2.358382
103.820063	1770.325095	5.322291	-0.020537	2.363216
104.185913	1778.389209	5.327296	-0.020611	2.368067
104.591677	1786.426766	5.332301	-0.020691	2.372895
104.900210	1794.500598	5.337306	-0.020754	2.377727
104.807546	1802.595445	5.342310	-0.020743	2.382529
105.149230	1810.632586	5.347315	-0.020812	2.387322
105.536081	1818.722060	5.352320	-0.020889	2.392140
105.525602	1826.794393	5.357325	-0.020893	2.396907
105.832800	1834.830361	5.362330	-0.020955	2.401667
106.075582	1842.898237	5.367334	-0.021006	2.406432
106.539020	1850.936434	5.372339	-0.021098	2.411188
106.868850	1859.021887	5.377344	-0.021165	2.415951
106.862553	1867.097008	5.382349	-0.021169	2.420672
107.183375	1875.147811	5.387354	-0.021234	2.425396
107.527929	1883.222121	5.392358	-0.021304	2.430125
107.562951	1891.389538	5.397363	-0.021316	2.434876
107.994141	1899.385807	5.402368	-0.021401	2.439549
107.920167	1907.447714	5.407373	-0.021393	2.444212
108.202268	1915.479813	5.412378	-0.021451	2.448876
108.821682	1923.512682	5.417382	-0.021572	2.453557
109.006581	1931.572908	5.422387	-0.021612	2.458211
109.438162	1939.633128	5.427392	-0.021697	2.462876
109.704117	1947.678521	5.432397	-0.021752	2.467511
110.060597	1955.758801	5.437402	-0.021824	2.472164
110.409133	1963.825498	5.442406	-0.021894	2.476799
110.412083	1971.874677	5.447411	-0.021900	2.481390
110.680226	1979.946335	5.452416	-0.021956	2.486005
110.983275	1987.988779	5.457421	-0.022018	2.490598
111.145983	1996.082616	5.462426	-0.022053	2.495201
111.432781	2004.120001	5.467430	-0.022112	2.499772
111.693692	2012.143281	5.472435	-0.022166	2.504325
112.024940	2020.220469	5.477440	-0.022233	2.508905
112.351388	2028.291886	5.482445	-0.022300	2.513474
112.774367	2036.343562	5.487450	-0.022384	2.518030
113.112431	2044.363335	5.492454	-0.022452	2.522553
113.110053	2052.426539	5.497459	-0.022457	2.527068
113.621984	2060.457129	5.502464	-0.022558	2.531594
113.774236	2068.540502	5.507469	-0.022592	2.536115
113.938235	2076.609979	5.512474	-0.022628	2.540621
114.306214	2084.634488	5.517478	-0.022702	2.545109
114.524396	2092.702571	5.522483	-0.022748	2.549602
115.029783	2100.761557	5.527488	-0.022847	2.554103
115.173414	2108.808030	5.532493	-0.022879	2.558563
115.666983	2116.841350	5.537498	-0.022977	2.563033
115.733037	2124.911540	5.542502	-0.022994	2.567485
115.695760	2133.005412	5.547507	-0.022993	2.571936
116.071138	2141.082948	5.552512	-0.023068	2.576398
116.193228	2149.123932	5.557517	-0.023097	2.580815
116.390671	2157.151618	5.562522	-0.023139	2.585222
116.643515	2165.230509	5.567526	-0.023191	2.589654
116.957253	2173.452414	5.572531	-0.023255	2.594160
117.452166	2181.431179	5.577536	-0.023353	2.598538
117.642083	2189.416056	5.582541	-0.023394	2.602891
117.681736	2197.469415	5.587546	-0.023406	2.607264
118.011667	2205.492441	5.592550	-0.023473	2.611633
118.175766	2213.529480	5.597555	-0.023509	2.615991
118.726557	2221.527748	5.602560	-0.023617	2.620346
118.801312	2229.585831	5.607565	-0.023636	2.624695
118.919636	2237.662109	5.612570	-0.023664	2.629049
119.209563	2245.718760	5.617574	-0.023723	2.633397
119.315945	2253.771322	5.622579	-0.023749	2.637723
119.733917	2261.775220	5.627584	-0.023832	2.642036
119.861205	2269.820553	5.632589	-0.023861	2.646346
120.318741	2277.864353	5.637594	-0.023952	2.650669
120.415033	2285.959335	5.642598	-0.023975	2.654989
120.443329	2294.008628	5.647603	-0.023986	2.659273
120.740064	2302.051113	5.652608	-0.024046	2.663564
120.933171	2310.082842	5.657613	-0.024088	2.667835
121.229197	2318.166985	5.662618	-0.024148	2.672134
121.638936	2326.221555	5.667622	-0.024230	2.676418
121.939452	2334.224366	5.672627	-0.024291	2.680660
122.401225	2342.247798	5.677632	-0.024383	2.684917
122.487326	2350.297567	5.682637	-0.024404	2.689157
122.693035	2358.384933	5.687642	-0.024448	2.693418
122.896871	2366.431236	5.692646	-0.024491	2.697650
122.913406	2374.476424	5.697651	-0.024500	2.701863
123.559454	2382.486099	5.702656	-0.024626	2.706091
123.601137	2390.565563	5.707661	-0.024639	2.710310
123.647776	2398.647463	5.712666	-0.024653	2.714524
124.154135	2406.657006	5.717670	-0.024753	2.718723
124.244722	2414.678905	5.722675	-0.024775	2.722896
124.581750	2422.732615	5.727680	-0.024843	2.727094
124.820077	2430.778697	5.732685	-0.024893	2.731276
125.102578	2438.842284	5.737690	-0.024951	2.735463
124.965738	2446.920282	5.742694	-0.024931	2.739625
125.086525	2454.929105	5.747699	-0.024959	2.743761
125.361234	2462.988359	5.752704	-0.025015	2.747926
125.886249	2471.045689	5.757709	-0.025119	2.752099
126.115054	2479.143730	5.762714	-0.025167	2.756268
126.347388	2487.154365	5.767718	-0.025215	2.760387
126.649181	2495.136587	5.772723	-0.025277	2.764489
127.003059	2503.185290	5.777728	-0.025348	2.768622
127.018215	2511.253989	5.782733	-0.025357	2.772739
127.189509	2519.301132	5.787738	-0.025394	2.776847
127.578733	2527.326298	5.792742	-0.025472	2.780952
127.679135	2535.351012	5.797747	-0.025496	2.785033
128.071633	2543.391215	5.802752	-0.025574	2.789133
128.316194	2551.456315	5.807757	-0.025625	2.793231
128.395372	2559.508058	5.812762	-0.025646	2.797307
128.637395	2567.542253	5.817766	-0.025696	2.801377
128.974634	2575.532047	5.822771	-0.025764	2.805424
129.127857	2583.614977	5.827776	-0.025798	2.809502
129.271449	2591.684124	5.832781	-0.025830	2.813566
129.713806	2599.700850	5.837786	-0.025918	2.817615
130.360022	2607.703507	5.842790	-0.026044	2.821663
130.282991	2615.770802	5.847795	-0.026035	2.825696
130.598514	2623.823509	5.852800	-0.026099	2.829739
131.080937	2631.878902	5.857805	-0.026195	2.833786
131.279742	2639.914419	5.862810	-0.026237	2.837801
131.307974	2647.978306	5.867814	-0.026248	2.841816
131.486894	2655.991256	5.872819	-0.026286	2.845807
132.060531	2664.008015	5.877824	-0.026399	2.849818
132.132399	2672.082392	5.882829	-0.026417	2.853823
132.334869	2680.107329	5.887834	-0.026461	2.857805
132.593384	2688.171408	5.892838	-0.026514	2.861804
132.884251	2696.183759	5.897843	-0.026574	2.865773
133.228015	2704.225544	5.902848	-0.026643	2.869755
133.499600	2712.290591	5.907853	-0.026699	2.873738
133.618770	2720.323632	5.912858	-0.026727	2.877692
133.995094	2728.347990	5.917862	-0.026802	2.881650
134.186831	2736.374205	5.922867	-0.026843	2.885593
134.508687	2744.443638	5.927872	-0.026909	2.889560
134.573311	2752.510721	5.932877	-0.026926	2.893505
134.708034	2760.542673	5.937882	-0.026957	2.897432
134.934350	2768.606875	5.942886	-0.027004	2.901374
134.878082	2776.621604	5.947891	-0.026999	2.905272
135.117182	2784.674915	5.952896	-0.027049	2.909199
135.160640	2792.793615	5.957901	-0.027063	2.913141
135.738082	2800.793750	5.962906	-0.027176	2.917050
135.849457	2808.808311	5.967910	-0.027202	2.920935
136.148468	2816.780745	5.972915	-0.027263	2.924805
136.515392	2824.814722	5.977920	-0.027337	2.928703
136.580665	2832.868552	5.982925	-0.027354	2.932589
136.806220	2840.918242	5.987930	-0.027402	2.936476
137.170744	2848.923333	5.992934	-0.027475	2.940345
137.377085	2856.938772	5.997939	-0.027519	2.944204
137.786216	2864.991080	6.002944	-0.027600	2.948087
138.005982	2873.036879	6.007949	-0.027647	2.951952
138.281383	2881.104323	6.012954	-0.027703	2.955825
138.479507	2889.135892	6.017958	-0.027746	2.959671
138.626771	2897.158609	6.022963	-0.027779	2.963506
138.767829	2905.218042	6.027968	-0.027810	2.967353
138.772638	2913.278985	6.032973	-0.027817	2.971189
138.876933	2921.310126	6.037978	-0.027842	2.975010
139.210298	2929.329166	6.042982	-0.027909	2.978833
139.474210	2937.348299	6.047987	-0.027964	2.982647
139.716026	2945.385474	6.052992	-0.028014	2.986464
139.823047	2953.438792	6.057997	-0.028039	2.990276
140.259660	2961.476111	6.063002	-0.028126	2.994093
140.594740	2969.502867	6.068006	-0.028194	2.997895
140.521434	2977.538687	6.073011	-0.028186	3.001675
140.820629	2985.570574	6.078016	-0.028247	3.005468
141.194791	2993.568968	6.083021	-0.028322	3.009244
141.311598	3001.644598	6.088026	-0.028349	3.013038
141.638391	3009.688459	6.093030	-0.028415	3.016823
141.895371	3017.678477	6.098035	-0.028469	3.020575
142.293376	3025.698596	6.103040	-0.028548	3.024343
142.615044	3033.746929	6.108045	-0.028613	3.028116
142.893179	3041.793253	6.113050	-0.028671	3.031880
142.998028	3049.901947	6.118054	-0.028696	3.035661
143.120287	3057.875926	6.123059	-0.028724	3.039375
143.490373	3065.912102	6.128064	-0.028798	3.043126
143.665329	3073.946222	6.133069	-0.028836	3.046861
144.065046	3081.971174	6.138074	-0.028916	3.050599
144.275684	3090.042513	6.143078	-0.028961	3.054344
144.477664	3098.046362	6.148083	-0.029004	3.058053
144.674374	3106.096445	6.153088	-0.029046	3.061778
144.928417	3114.120765	6.158093	-0.029098	3.065490
145.237771	3122.147264	6.163098	-0.029162	3.069201
145.313414	3130.288290	6.168102	-0.029181	3.072949
145.306936	3138.332730	6.173107	-0.029185	3.076644
145.493988	3146.335198	6.178112	-0.029226	3.080325
145.688908	3154.316550	6.183117	-0.029267	3.083991
145.957000	3162.316485	6.188122	-0.029323	3.087666
146.304344	3170.379590	6.193126	-0.029393	3.091368
146.525528	3178.420791	6.198131	-0.029439	3.095050
146.659200	3186.457200	6.203136	-0.029470	3.098722
146.988646	3194.461624	6.208141	-0.029536	3.102383
147.402966	3202.476103	6.213146	-0.029619	3.106049
147.674553	3210.525535	6.218150	-0.029675	3.109719
147.898335	3218.565306	6.223155	-0.029722	3.113379
148.280199	3226.597539	6.228160	-0.029799	3.117038
148.565523	3234.625551	6.233165	-0.029857	3.120686
148.712917	3242.600133	6.238170	-0.029890	3.124300
148.927774	3250.674842	6.243174	-0.029935	3.127958
149.316209	3258.696974	6.248179	-0.030013	3.131595
149.582078	3266.767058	6.253184	-0.030068	3.135244
149.719351	3274.803834	6.258189	-0.030099	3.138869
149.925146	3282.810595	6.263194	-0.030143	3.142478
150.135978	3290.890164	6.268198	-0.030187	3.146117
150.178571	3298.885646	6.273203	-0.030201	3.149706
150.595599	3306.972222	6.278208	-0.030284	3.153348
150.634909	3315.007465	6.283213	-0.030297	3.156946
150.695604	3323.003012	6.288218	-0.030313	3.160524
150.868758	3331.012830	6.293222	-0.030351	3.164108
151.006568	3339.042252	6.298227	-0.030382	3.167696
151.306883	3347.091084	6.303232	-0.030443	3.171296
151.360100	3355.146384	6.308237	-0.030459	3.174883
151.575731	3363.146008	6.313242	-0.030504	3.178449
151.919393	3371.194485	6.318246	-0.030574	3.182038
152.040657	3379.201717	6.323251	-0.030602	3.185594
152.438696	3387.245770	6.328256	-0.030681	3.189175
152.640776	3395.295902	6.333261	-0.030724	3.192747
152.842257	3403.337546	6.338266	-0.030767	3.196310
153.215203	3411.320325	6.343270	-0.030842	3.199851
153.321761	3419.345208	6.348275	-0.030867	3.203395
153.528469	3427.397914	6.353280	-0.030911	3.206951
153.726665	3435.431372	6.358285	-0.030954	3.210495
153.848272	3443.475351	6.363290	-0.030982	3.214036
154.350531	3451.507380	6.368294	-0.031081	3.217584
154.322593	3459.552753	6.373299	-0.031081	3.221112
154.406944	3467.545084	6.378304	-0.031102	3.224618
154.846868	3475.557150	6.383309	-0.031189	3.228142
155.042166	3483.643901	6.388314	-0.031231	3.231686
155.108382	3491.738781	6.393318	-0.031249	3.235224
155.291747	3499.694188	6.398323	-0.031288	3.238702
155.510545	3507.720906	6.403328	-0.031335	3.242208
155.780285	3515.717984	6.408333	-0.031390	3.245700
155.854116	3523.736882	6.413338	-0.031409	3.249190
156.166041	3531.810818	6.418342	-0.031473	3.252709
156.270873	3539.842154	6.423347	-0.031498	3.256198
156.481882	3547.841425	6.428352	-0.031543	3.259674
156.969536	3555.854307	6.433357	-0.031639	3.263162
157.085872	3563.896224	6.438362	-0.031666	3.266645
157.213321	3571.947943	6.443366	-0.031695	3.270128
157.432843	3580.007176	6.448371	-0.031741	3.273615
157.757313	3588.033703	6.453376	-0.031807	3.277088
157.795374	3596.051342	6.458381	-0.031820	3.280542
158.215814	3604.024001	6.463386	-0.031903	3.283988
158.699554	3612.077314	6.468390	-0.031999	3.287468
159.036845	3620.100921	6.473395	-0.032067	3.290925
159.165994	3628.179516	6.478400	-0.032097	3.294394
159.378466	3636.198703	6.483405	-0.032142	3.297837
159.703065	3644.199563	6.488410	-0.032207	3.301273
159.816285	3652.214634	6.493414	-0.032234	3.304704
159.877054	3660.256665	6.498419	-0.032251	3.308140
159.961396	3668.333559	6.503424	-0.032272	3.311589
160.201746	3676.374300	6.508429	-0.032322	3.315024
160.415940	3684.335563	6.513434	-0.032367	3.318421
160.736591	3692.375027	6.518438	-0.032432	3.321852
160.816632	3700.375038	6.523443	-0.032453	3.325253
161.150656	3708.392615	6.528448	-0.032520	3.328668
161.433634	3716.451069	6.533453	-0.032578	3.332095
161.490530	3724.506765	6.538458	-0.032594	3.335509
161.578224	3732.528188	6.543462	-0.032616	3.338905
161.684584	3740.538464	6.548467	-0.032641	3.342295
162.187035	3748.563936	6.553472	-0.032740	3.345701
162.393368	3756.604258	6.558477	-0.032784	3.349100
162.504534	3764.629951	6.563482	-0.032810	3.352485
162.679155	3772.722161	6.568486	-0.032848	3.355898
162.897421	3780.687449	6.573491	-0.032894	3.359255
163.057611	3788.726041	6.578496	-0.032930	3.362637
163.331977	3796.741434	6.583501	-0.032986	3.366011
163.548258	3804.734953	6.588506	-0.033032	3.369369
163.921280	3812.819398	6.593510	-0.033107	3.372768
164.031915	3820.858371	6.598515	-0.033133	3.376135
164.559568	3828.846830	6.603520	-0.033236	3.379493
164.751128	3836.886194	6.608525	-0.033277	3.382856
164.949444	3844.918858	6.613530	-0.033320	3.386213
165.267468	3852.949495	6.618534	-0.033384	3.389571
165.377266	3861.047802	6.623539	-0.033410	3.392946
165.506820	3869.093234	6.628544	-0.033440	3.396296
165.794846	3877.019115	6.633549	-0.033499	3.399599
166.024706	3885.040495	6.638554	-0.033547	3.402936
166.237241	3893.090144	6.643558	-0.033592	3.406281
166.294125	3901.085355	6.648563	-0.033608	3.409594
166.527992	3909.129543	6.653568	-0.033657	3.412931
166.851012	3917.162249	6.658573	-0.033723	3.416263
166.794063	3925.165526	6.663578	-0.033717	3.419566
167.255291	3933.191345	6.668582	-0.033809	3.422893
167.442792	3941.207545	6.673587	-0.033849	3.426204
167.418553	3949.277788	6.678592	-0.033850	3.429526
167.619352	3957.316175	6.683597	-0.033893	3.432840
167.924926	3965.329557	6.688602	-0.033955	3.436144
168.191708	3973.333421	6.693606	-0.034010	3.439439
168.393212	3981.308516	6.698611	-0.034053	3.442717
168.478949	3989.395212	6.703616	-0.034075	3.446034
168.610507	3997.418139	6.708621	-0.034104	3.449323
168.711675	4005.463464	6.713626	-0.034129	3.452617
169.091148	4013.508651	6.718630	-0.034205	3.455917
169.252648	4021.517238	6.723635	-0.034240	3.459192
169.463540	4029.560940	6.728640	-0.034285	3.462479
169.773875	4037.569185	6.733645	-0.034348	3.465752
170.032456	4045.573162	6.738650	-0.034402	3.469019
170.199899	4053.672703	6.743654	-0.034438	3.472318
170.376544	4061.680900	6.748659	-0.034477	3.475578
170.500671	4069.708553	6.753664	-0.034505	3.478840
170.704713	4077.718244	6.758669	-0.034549	3.482095
170.753658	4085.665249	6.763674	-0.034563	3.485316
171.082752	4093.714157	6.768678	-0.034630	3.488584
171.404332	4101.731970	6.773683	-0.034695	3.491837
171.538345	4109.790627	6.778688	-0.034725	3.495097
171.633973	4117.824272	6.783693	-0.034749	3.498343
171.788052	4125.823706	6.788698	-0.034783	3.501573
172.054810	4133.838147	6.793702	-0.034838	3.504810
172.336805	4141.844205	6.798707	-0.034896	3.508042
172.712145	4149.887863	6.803712	-0.034971	3.511288
172.826702	4157.947556	6.808717	-0.034998	3.514530
172.826665	4165.955849	6.813722	-0.035003	3.517744
173.159484	4173.995831	6.818726	-0.035071	3.520978
173.379991	4181.983340	6.823731	-0.035117	3.524185
173.603202	4190.025627	6.828736	-0.035164	3.527411
173.657173	4198.071066	6.833741	-0.035180	3.530630
173.879395	4206.096272	6.838746	-0.035226	3.533844
173.956467	4214.154734	6.843750	-0.035246	3.537063
173.986667	4222.165376	6.848755	-0.035257	3.540258
174.826429	4230.121596	6.853760	-0.035419	3.543454
175.226499	4238.180363	6.858765	-0.035499	3.546674
175.468177	4246.197242	6.863770	-0.035549	3.549869
175.798980	4254.345296	6.868774	-0.035616	3.553117
176.231652	4262.348616	6.873779	-0.035702	3.556307
176.252826	4270.333177	6.878784	-0.035712	3.559475
176.504199	4278.360632	6.883789	-0.035764	3.562663
176.562122	4286.351308	6.888794	-0.035780	3.565828
176.578341	4294.389301	6.893798	-0.035789	3.569009
176.549768	4302.414059	6.898803	-0.035789	3.572179
177.141172	4310.410799	6.903808	-0.035904	3.575354
177.417650	4318.425269	6.908813	-0.035961	3.578524
177.385242	4326.463943	6.913818	-0.035960	3.581691
177.581096	4334.474099	6.918822	-0.036002	3.584851
177.634649	4342.481889	6.923827	-0.036018	3.588004
177.934443	4350.533774	6.928832	-0.036079	3.591178
178.181994	4358.552953	6.933837	-0.036130	3.594334
178.152536	4366.576139	6.938842	-0.036130	3.597482
178.579121	4374.585591	6.943846	-0.036215	3.600634
178.434116	4382.593707	6.948851	-0.036194	3.603767
178.728475	4390.641238	6.953856	-0.036254	3.606925
179.051649	4398.634008	6.958861	-0.036319	3.610059
179.133955	4406.690136	6.963866	-0.036340	3.613209
179.542251	4414.745482	6.968870	-0.036422	3.616365
179.744051	4422.729724	6.973875	-0.036465	3.619484
179.929341	4430.752573	6.978880	-0.036505	3.622616
179.897989	4438.763157	6.983885	-0.036504	3.625734
180.329512	4446.776348	6.988890	-0.036590	3.628863
180.629072	4454.872566	6.993894	-0.036651	3.632017
180.670374	4462.926369	6.998899	-0.036664	3.635146
180.945024	4470.938747	7.003904	-0.036721	3.638262
181.138200	4478.999213	7.008909	-0.036762	3.641392
181.382289	4486.903525	7.013914	-0.036813	3.644460
181.582070	4494.985539	7.018918	-0.036856	3.647593
181.902906	4502.991169	7.023923	-0.036921	3.650697
182.212447	4511.035260	7.028928	-0.036984	3.653812
182.286664	4519.112123	7.033933	-0.037003	3.656932
182.258205	4527.066847	7.038938	-0.037003	3.659999
182.698907	4535.077478	7.043942	-0.037091	3.663097
182.976092	4543.088304	7.048947	-0.037148	3.666189
183.213411	4551.115207	7.053952	-0.037197	3.669283
183.435982	4559.179245	7.058957	-0.037244	3.672388
183.539873	4567.180092	7.063962	-0.037269	3.675463
183.817216	4575.216800	7.068966	-0.037326	3.678554
184.108022	4583.239133	7.073971	-0.037386	3.681637
184.232462	4591.222306	7.078976	-0.037414	3.684698
184.371475	4599.274868	7.083981	-0.037445	3.687783
184.586259	4607.258180	7.088986	-0.037491	3.690842
185.003814	4615.328867	7.093990	-0.037574	3.693936
184.863786	4623.333502	7.098995	-0.037553	3.696988
184.994280	4631.345817	7.104000	-0.037583	3.700048
185.317352	4639.363730	7.109005	-0.037649	3.703112
185.479389	4647.380052	7.114010	-0.037684	3.706168
185.730006	4655.440008	7.119014	-0.037736	3.709241
185.900156	4663.511151	7.124019	-0.037773	3.712314
186.099869	4671.586335	7.129024	-0.037816	3.715386
186.210049	4679.538279	7.134029	-0.037842	3.718407
186.249499	4687.533399	7.139034	-0.037855	3.721440
186.570949	4695.524459	7.144038	-0.037920	3.724476
186.439316	4703.551885	7.149043	-0.037901	3.727512
186.607436	4711.540344	7.154048	-0.037938	3.730538
186.980890	4719.602514	7.159053	-0.038013	3.733595
187.094782	4727.646504	7.164058	-0.038039	3.736636
187.300382	4735.649123	7.169062	-0.038083	3.739661
187.714471	4743.631983	7.174067	-0.038165	3.742681
188.134852	4751.669997	7.179072	-0.038249	3.745719
188.433978	4759.703210	7.184077	-0.038310	3.748750
188.550674	4767.724513	7.189082	-0.038337	3.751770
188.832452	4775.815237	7.194086	-0.038395	3.754817
189.146605	4783.757634	7.199091	-0.038459	3.757807
189.074560	4791.830167	7.204096	-0.038451	3.760835
189.314327	4799.850054	7.209101	-0.038501	3.763847
189.494782	4807.825084	7.214106	-0.038540	3.766839
189.698195	4815.883570	7.219110	-0.038584	3.769860
189.756946	4823.918167	7.224115	-0.038600	3.772867
189.927322	4831.950770	7.229120	-0.038637	3.775872
190.110163	4839.962338	7.234125	-0.038676	3.778868
190.259509	4847.970650	7.239130	-0.038710	3.781860
190.561943	4855.982888	7.244134	-0.038771	3.784854
190.575378	4864.015547	7.249139	-0.038779	3.787847
190.801745	4872.031805	7.254144	-0.038827	3.790836
190.961749	4880.127298	7.259149	-0.038862	3.793850
191.332873	4888.091584	7.264154	-0.038937	3.796818
191.271982	4896.109647	7.269158	-0.038931	3.799794
191.312040	4904.106994	7.274163	-0.038944	3.802763
191.444134	4912.126274	7.279168	-0.038974	3.805739
191.699530	4920.149747	7.284173	-0.039027	3.808717
191.691127	4928.178959	7.289178	-0.039030	3.811689
191.936898	4936.190393	7.294182	-0.039082	3.814658
192.207315	4944.229571	7.299187	-0.039137	3.817635
192.664841	4952.186553	7.304192	-0.039228	3.820584
192.712608	4960.260619	7.309197	-0.039242	3.823564
192.869534	4968.247517	7.314202	-0.039277	3.826513
193.093127	4976.303810	7.319206	-0.039324	3.829486
193.189192	4984.317736	7.324211	-0.039347	3.832438
193.416074	4992.373770	7.329216	-0.039395	3.835407
193.467559	5000.377243	7.334221	-0.039410	3.838350
193.286125	5008.396607	7.339226	-0.039382	3.841292
193.934528	5016.377171	7.344230	-0.039508	3.844234
194.052168	5024.398083	7.349235	-0.039535	3.847178
194.262289	5032.430270	7.354240	-0.039580	3.850126
194.527979	5040.480125	7.359245	-0.039634	3.853079
194.709212	5048.524735	7.364250	-0.039674	3.856026
194.755069	5056.542048	7.369254	-0.039688	3.858958
194.876999	5064.553612	7.374259	-0.039716	3.861888
194.999209	5072.560181	7.379264	-0.039744	3.864813
195.329274	5080.589788	7.384269	-0.039811	3.867749
195.214306	5088.616428	7.389274	-0.039795	3.870672
195.519426	5096.857002	7.394278	-0.039857	3.873679
195.755724	5104.842662	7.399283	-0.039907	3.876590
195.745125	5112.769561	7.404288	-0.039910	3.879473
196.096049	5120.771506	7.409293	-0.039981	3.882388
196.382769	5128.734025	7.414298	-0.040039	3.885285
196.543655	5136.760957	7.419302	-0.040075	3.888200
196.631037	5144.770323	7.424307	-0.040096	3.891106
196.826576	5152.803284	7.429312	-0.040138	3.894020
197.221739	5160.804241	7.434317	-0.040217	3.896924
197.329658	5168.777193	7.439322	-0.040243	3.899810
197.787881	5176.838031	7.444326	-0.040334	3.902733
197.886557	5184.858113	7.449331	-0.040357	3.905632
197.994965	5192.848221	7.454336	-0.040383	3.908518
198.177997	5200.925296	7.459341	-0.040422	3.911434
198.346463	5208.923444	7.464346	-0.040459	3.914320
198.557185	5216.978308	7.469350	-0.040504	3.917225
198.721119	5224.942700	7.474355	-0.040540	3.920094
198.685357	5232.996986	7.479360	-0.040539	3.922989
199.043415	5241.019007	7.484365	-0.040611	3.925878
199.213252	5248.988753	7.489370	-0.040648	3.928743
199.422897	5257.066849	7.494374	-0.040692	3.931645
199.893869	5265.085655	7.499379	-0.040785	3.934529
199.950690	5273.098962	7.504384	-0.040801	3.937401
200.199295	5281.078959	7.509389	-0.040853	3.940262
200.346377	5289.075133	7.514394	-0.040886	3.943125
200.623162	5297.080403	7.519398	-0.040943	3.945992
200.589763	5305.121719	7.524403	-0.040942	3.948864
200.760080	5313.197413	7.529408	-0.040979	3.951750
200.919614	5321.269984	7.534413	-0.041014	3.954632
201.004760	5329.252241	7.539418	-0.041035	3.957478
201.376695	5337.213274	7.544422	-0.041110	3.960320
201.424635	5345.226501	7.549427	-0.041124	3.963173
201.643731	5353.220638	7.554432	-0.041171	3.966020
201.769748	5361.247033	7.559437	-0.041199	3.968875
202.030368	5369.315957	7.564442	-0.041253	3.971745
202.127985	5377.358075	7.569446	-0.041277	3.974601
202.409549	5385.352436	7.574451	-0.041335	3.977441
202.268299	5393.376904	7.579456	-0.041314	3.980282
202.539753	5401.408032	7.584461	-0.041370	3.983130
202.737723	5409.378732	7.589466	-0.041412	3.985954
202.876972	5417.449752	7.594470	-0.041444	3.988811
203.089303	5425.479057	7.599475	-0.041489	3.991651
203.244590	5433.496460	7.604480	-0.041523	3.994485
203.564391	5441.591753	7.609485	-0.041588	3.997346
203.475133	5449.537156	7.614490	-0.041577	4.000147
203.812209	5457.554711	7.619494	-0.041645	4.002977
203.901767	5465.541385	7.624499	-0.041667	4.005790
204.230241	5473.606399	7.629504	-0.041733	4.008633
204.460279	5481.666598	7.634509	-0.041782	4.011471
204.505594	5489.643965	7.639514	-0.041796	4.014275
204.508561	5497.707094	7.644518	-0.041802	4.017106
204.881578	5505.688335	7.649523	-0.041876	4.019912
204.992623	5513.710908	7.654528	-0.041902	4.022726
204.993769	5521.740409	7.659533	-0.041908	4.025539
205.318216	5529.706112	7.664538	-0.041974	4.028333
205.602417	5537.763148	7.669542	-0.042032	4.031156
205.780102	5545.870767	7.674547	-0.042071	4.033994
205.967217	5553.896167	7.679552	-0.042111	4.036800
206.243477	5561.842012	7.684557	-0.042168	4.039579
206.333017	5569.856026	7.689562	-0.042190	4.042376
206.295011	5577.813872	7.694566	-0.042188	4.045150
206.450031	5585.855061	7.699571	-0.042223	4.047954
206.761620	5593.856734	7.704576	-0.042286	4.050744
206.923358	5601.932281	7.709581	-0.042322	4.053556
206.885776	5609.896067	7.714586	-0.042320	4.056324
207.338080	5617.911462	7.719590	-0.042410	4.059116
207.385366	5625.954707	7.724595	-0.042424	4.061909
207.379872	5633.949878	7.729600	-0.042428	4.064683
207.800791	5641.972693	7.734605	-0.042512	4.067471
207.835571	5649.973661	7.739610	-0.042524	4.070243
207.881741	5658.021138	7.744614	-0.042538	4.073030
208.330543	5666.041658	7.749619	-0.042627	4.075812
208.579001	5674.026219	7.754624	-0.042679	4.078576
208.874311	5682.060532	7.759629	-0.042739	4.081356
208.776305	5690.050070	7.764634	-0.042726	4.084113
209.050436	5698.087267	7.769638	-0.042783	4.086890
209.278768	5706.088382	7.774643	-0.042830	4.089652
209.131393	5714.126045	7.779648	-0.042808	4.092420
209.509041	5722.191251	7.784653	-0.042884	4.095202
209.705427	5730.172937	7.789658	-0.042926	4.097952
209.740786	5738.225320	7.794662	-0.042938	4.100721
209.909008	5746.199910	7.799667	-0.042975	4.103464
210.257789	5754.226668	7.804672	-0.043045	4.106225
210.484990	5762.266333	7.809677	-0.043093	4.108987
210.401350	5770.313250	7.814682	-0.043083	4.111746
210.841072	5778.360432	7.819686	-0.043170	4.114509
210.911407	5786.375064	7.824691	-0.043189	4.117255
211.127865	5794.325768	7.829696	-0.043234	4.119979
211.361417	5802.362463	7.834701	-0.043283	4.122731
211.781507	5810.330143	7.839706	-0.043367	4.125459
211.836503	5818.393465	7.844710	-0.043383	4.128214
212.032982	5826.415873	7.849715	-0.043425	4.130955
212.222457	5834.448530	7.854720	-0.043465	4.133697
212.343333	5842.544052	7.859725	-0.043493	4.136458
212.538313	5850.470945	7.864730	-0.043535	4.139161
212.773720	5858.553950	7.869734	-0.043584	4.141916
213.027142	5866.460038	7.874739	-0.043637	4.144608
213.221774	5874.546151	7.879744	-0.043678	4.147360
213.313450	5882.578828	7.884749	-0.043701	4.150090
213.661679	5890.598689	7.889754	-0.043771	4.152817
213.979871	5898.614891	7.894758	-0.043836	4.155541
214.193533	5906.638256	7.899763	-0.043881	4.158264
214.420943	5914.625951	7.904768	-0.043929	4.160973
214.790148	5922.648240	7.909773	-0.044003	4.163694
214.785478	5930.677544	7.914778	-0.044007	4.166411
215.181391	5938.704126	7.919782	-0.044087	4.169130
215.508908	5946.720855	7.924787	-0.044153	4.171843
215.456839	5954.737104	7.929792	-0.044149	4.174550
215.854371	5962.772326	7.934797	-0.044228	4.177266
216.138918	5970.745378	7.939802	-0.044286	4.179959
216.382792	5978.789883	7.944806	-0.044337	4.182673
216.238291	5986.777268	7.949811	-0.044316	4.185362
216.404252	5994.783812	7.954816	-0.044352	4.188059
216.558963	6002.868365	7.959821	-0.044386	4.190780
216.424013	6010.941495	7.964826	-0.044367	4.193493
216.818034	6018.976969	7.969830	-0.044446	4.196197
217.049302	6026.917831	7.974835	-0.044494	4.198866
216.879464	6034.913666	7.979840	-0.044468	4.201547
217.240468	6042.906369	7.984845	-0.044540	4.204231
217.440280	6050.889761	7.989850	-0.044583	4.206908
217.456718	6058.898899	7.994854	-0.044591	4.209591
217.456351	6066.986457	7.999859	-0.044597	4.212298
217.811376	6074.980645	8.004864	-0.044668	4.214975
217.871752	6083.071195	8.009869	-0.044685	4.217680
217.925536	6090.971770	8.014874	-0.044700	4.220320
218.218329	6099.036711	8.019878	-0.044760	4.223015
218.566138	6107.034156	8.024883	-0.044830	4.225686
218.610253	6115.025147	8.029888	-0.044844	4.228351
218.898062	6123.091873	8.034893	-0.044903	4.231041
218.915353	6131.089182	8.039898	-0.044912	4.233704
219.013476	6139.196199	8.044902	-0.044935	4.236403
219.206234	6147.121656	8.049907	-0.044977	4.239041
219.357932	6155.146333	8.054912	-0.045010	4.241709
219.541713	6163.114107	8.059917	-0.045050	4.244357
219.583114	6171.184085	8.064922	-0.045063	4.247036
219.703450	6179.179780	8.069926	-0.045091	4.249689
220.065659	6187.239777	8.074931	-0.045164	4.252365
220.088528	6195.237979	8.079936	-0.045173	4.255015
220.440145	6203.300124	8.084941	-0.045244	4.257687
220.658792	6211.269153	8.089946	-0.045290	4.260326
220.830856	6219.305862	8.094950	-0.045328	4.262985
220.622895	6227.325688	8.099955	-0.045295	4.265633
220.872424	6235.341125	8.104960	-0.045347	4.268283
221.196019	6243.392819	8.109965	-0.045412	4.270943
221.183757	6251.435725	8.114970	-0.045415	4.273596
221.451474	6259.486792	8.119974	-0.045471	4.276252
221.649355	6267.460407	8.124979	-0.045513	4.278880
221.655318	6275.445812	8.129984	-0.045519	4.281509
222.040424	6283.423676	8.134989	-0.045596	4.284137
222.079992	6291.463733	8.139994	-0.045609	4.286781
222.130013	6299.503766	8.144998	-0.045624	4.289424
222.292813	6307.567863	8.150003	-0.045660	4.292073
222.387649	6315.528309	8.155008	-0.045683	4.294687
222.697128	6323.638852	8.160013	-0.045746	4.297350
222.662408	6331.548524	8.165018	-0.045745	4.299942
223.038530	6339.593238	8.170022	-0.045820	4.302581
222.979672	6347.610478	8.175027	-0.045815	4.305205
223.195347	6355.605115	8.180032	-0.045860	4.307822
223.468655	6363.653024	8.185037	-0.045917	4.310456
223.510713	6371.677893	8.190042	-0.045930	4.313079
223.721635	6379.698048	8.195046	-0.045975	4.315700
223.673901	6387.740557	8.200051	-0.045971	4.318325
223.751335	6395.680760	8.205056	-0.045991	4.320915
224.124497	6403.710138	8.210061	-0.046066	4.323535
224.514107	6411.688584	8.215066	-0.046144	4.326138
224.644560	6419.697853	8.220070	-0.046173	4.328746
224.844630	6427.817023	8.225075	-0.046216	4.331390
224.998552	6435.820281	8.230080	-0.046250	4.333994
225.358117	6443.842266	8.235085	-0.046323	4.336603
225.612523	6451.796476	8.240090	-0.046375	4.339189
225.854598	6459.830841	8.245094	-0.046426	4.341798
225.917097	6467.823835	8.250099	-0.046443	4.344392
225.908671	6475.863561	8.255104	-0.046447	4.346998
226.089901	6483.901340	8.260109	-0.046486	4.349604
226.270260	6491.941145	8.265114	-0.046525	4.352209
226.442957	6500.051619	8.270118	-0.046562	4.354834
226.547334	6508.040971	8.275123	-0.046587	4.357419
226.745627	6515.919263	8.280128	-0.046630	4.359967
227.015451	6523.967127	8.285133	-0.046685	4.362569
226.953646	6531.943130	8.290138	-0.046679	4.365143
227.278523	6539.988053	8.295142	-0.046745	4.367741
227.470290	6548.009433	8.300147	-0.046786	4.370329
227.649344	6556.025231	8.305152	-0.046825	4.372913
228.070419	6564.055909	8.310157	-0.046909	4.375502
228.070928	6572.087591	8.315162	-0.046914	4.378088
228.152782	6580.089548	8.320166	-0.046935	4.380662
228.416528	6588.107557	8.325171	-0.046989	4.383242
228.391717	6596.083044	8.330176	-0.046990	4.385804
228.615059	6604.155110	8.335181	-0.047037	4.388398
228.888362	6612.122199	8.340186	-0.047093	4.390956
229.221573	6620.166045	8.345190	-0.047161	4.393538
229.307015	6628.243326	8.350195	-0.047182	4.396128
229.344495	6636.161477	8.355200	-0.047195	4.398665
229.656707	6644.239624	8.360205	-0.047258	4.401253
229.622208	6652.176096	8.365210	-0.047257	4.403792
230.021648	6660.257566	8.370214	-0.047337	4.406379
230.159293	6668.277791	8.375219	-0.047368	4.408943
230.271029	6676.290449	8.380224	-0.047394	4.411503
230.358354	6684.338519	8.385229	-0.047416	4.414073
230.500298	6692.358180	8.390234	-0.047448	4.416632
231.012943	6700.326966	8.395238	-0.047549	4.419176
230.903792	6708.416713	8.400243	-0.047534	4.421753
230.935156	6716.353159	8.405248	-0.047545	4.424281
231.270256	6724.433936	8.410253	-0.047613	4.426855
231.499163	6732.390531	8.415258	-0.047661	4.429387
231.557029	6740.494674	8.420262	-0.047677	4.431964
231.785428	6748.544166	8.425267	-0.047725	4.434523
231.985016	6756.524069	8.430272	-0.047768	4.437058
232.215841	6764.471789	8.435277	-0.047816	4.439582
232.310188	6772.542142	8.440282	-0.047839	4.442142
232.342591	6780.458436	8.445286	-0.047850	4.444652
232.607448	6788.540785	8.450291	-0.047905	4.447214
232.794517	6796.504648	8.455296	-0.047945	4.449736
233.061600	6804.654651	8.460301	-0.048001	4.452316
232.970764	6812.578979	8.465306	-0.047989	4.454823
233.109364	6820.633346	8.470310	-0.048020	4.457369
233.389290	6828.586882	8.475315	-0.048078	4.459883
233.623423	6836.652385	8.480320	-0.048127	4.462431
233.618689	6844.655135	8.485325	-0.048131	4.464956
233.750168	6852.670754	8.490330	-0.048161	4.467484
234.093793	6860.688571	8.495334	-0.048231	4.470013
234.482101	6868.739323	8.500339	-0.048308	4.472551
234.364251	6876.739840	8.505344	-0.048292	4.475069
234.352538	6884.760557	8.510349	-0.048295	4.477593
234.686120	6892.743434	8.515354	-0.048362	4.480105
234.968451	6900.728479	8.520358	-0.048420	4.482615
235.090965	6908.790328	8.525363	-0.048449	4.485148
235.092984	6916.757527	8.530368	-0.048454	4.487649
235.333394	6924.818413	8.535373	-0.048505	4.490180
235.437999	6932.832472	8.540378	-0.048530	4.492693
235.597452	6940.849557	8.545382	-0.048565	4.495206
235.677672	6948.876912	8.550387	-0.048585	4.497721
235.475723	6956.870440	8.555392	-0.048553	4.500223
235.944722	6964.921327	8.560397	-0.048646	4.502743
236.196390	6972.871935	8.565402	-0.048698	4.505230
236.313468	6980.915103	8.570407	-0.048725	4.507745
236.113972	6988.926427	8.575411	-0.048693	4.510247
236.307106	6996.998997	8.580416	-0.048735	4.512767
236.954590	7005.043587	8.585421	-0.048861	4.515279
236.882113	7013.007281	8.590426	-0.048853	4.517762
236.897300	7020.984705	8.595431	-0.048861	4.520248
237.275594	7028.984958	8.600435	-0.048937	4.522741
237.468020	7036.952974	8.605440	-0.048978	4.525222
237.693797	7045.010529	8.610445	-0.049025	4.527730
237.759172	7053.012458	8.615450	-0.049043	4.530219
237.682747	7061.101123	8.620455	-0.049034	4.532732
237.922890	7069.141002	8.625459	-0.049084	4.535230
238.132006	7077.086021	8.630464	-0.049129	4.537697
238.332993	7085.107965	8.635469	-0.049171	4.540187
238.398158	7093.140206	8.640474	-0.049189	4.542678
238.408526	7101.109684	8.645479	-0.049196	4.545148
238.771654	7109.176404	8.650483	-0.049269	4.547647
238.809044	7117.172715	8.655488	-0.049282	4.550123
238.943221	7125.240546	8.660493	-0.049312	4.552620
239.046027	7133.237282	8.665498	-0.049337	4.555093
239.142651	7141.270771	8.670503	-0.049360	4.557576
239.331878	7149.224384	8.675507	-0.049401	4.560034
239.472796	7157.282701	8.680512	-0.049432	4.562522
239.818588	7165.272823	8.685517	-0.049502	4.564988
240.071401	7173.315346	8.690522	-0.049555	4.567469
240.095712	7181.276032	8.695527	-0.049565	4.569923
240.571070	7189.381416	8.700531	-0.049659	4.572420
240.567592	7197.362101	8.705536	-0.049663	4.574878
240.665884	7205.443185	8.710541	-0.049687	4.577365
240.719643	7213.335925	8.715546	-0.049702	4.579792
240.959782	7221.451827	8.720551	-0.049753	4.582287
241.151795	7229.417875	8.725555	-0.049794	4.584735
241.170594	7237.388639	8.730560	-0.049803	4.587183
241.445614	7245.441516	8.735565	-0.049859	4.589654
241.394033	7253.527939	8.740570	-0.049855	4.592135
241.578909	7261.541951	8.745575	-0.049895	4.594592
241.740963	7269.579728	8.750579	-0.049931	4.597055
241.894554	7277.497493	8.755584	-0.049964	4.599480
242.094854	7285.573514	8.760589	-0.050007	4.601952
242.151870	7293.516273	8.765594	-0.050023	4.604381
242.416442	7301.605096	8.770599	-0.050078	4.606855
242.406189	7309.560537	8.775603	-0.050081	4.609286
242.716938	7317.599859	8.780608	-0.050145	4.611741
242.932719	7325.624162	8.785613	-0.050190	4.614191
242.961719	7333.644602	8.790618	-0.050201	4.616638
242.895244	7341.615006	8.795623	-0.050194	4.619068
243.152021	7349.677887	8.800627	-0.050247	4.621526
243.269428	7357.627168	8.805632	-0.050275	4.623947
243.489493	7365.699749	8.810637	-0.050321	4.626405
243.494113	7373.709765	8.815642	-0.050327	4.628842
243.927237	7381.741011	8.820647	-0.050413	4.631284
243.898015	7389.808844	8.825651	-0.050413	4.633737
243.830963	7397.824348	8.830656	-0.050406	4.636172
244.065175	7405.762349	8.835661	-0.050455	4.638582
244.129905	7413.769046	8.840666	-0.050473	4.641012
244.215498	7421.758400	8.845671	-0.050494	4.643435
244.655727	7429.810538	8.850675	-0.050581	4.645876
244.925135	7437.797579	8.855680	-0.050637	4.648296
245.121104	7445.830960	8.860685	-0.050679	4.650729
245.235489	7453.902428	8.865690	-0.050706	4.653171
245.212658	7461.896190	8.870695	-0.050707	4.655590
245.375680	7469.904050	8.875699	-0.050743	4.658011
245.511308	7477.864378	8.880704	-0.050773	4.660416
245.717806	7485.958390	8.885709	-0.050817	4.662861
245.803699	7493.914531	8.890714	-0.050838	4.665263
245.963589	7501.971380	8.895719	-0.050874	4.667693
246.364226	7509.957977	8.900723	-0.050954	4.670101
246.592431	7518.033016	8.905728	-0.051002	4.672535
246.561674	7526.157756	8.910733	-0.051001	4.674983
246.752318	7534.065916	8.915738	-0.051042	4.677364
247.225407	7541.996264	8.920743	-0.051136	4.679749
247.245078	7550.062322	8.925747	-0.051145	4.682176
247.329013	7557.956352	8.930752	-0.051166	4.684549
247.718741	7566.087963	8.935757	-0.051244	4.686991
247.714553	7574.039638	8.940762	-0.051248	4.689379
247.858668	7582.082643	8.945767	-0.051281	4.691793
248.124703	7590.120224	8.950771	-0.051336	4.694204
248.053902	7598.151497	8.955776	-0.051328	4.696612
248.253805	7606.131401	8.960781	-0.051370	4.699003
248.337968	7614.132369	8.965786	-0.051392	4.701400
248.376437	7622.149649	8.970791	-0.051404	4.703800
248.676927	7630.208461	8.975795	-0.051465	4.706211
248.815645	7638.161715	8.980800	-0.051497	4.708589
249.215363	7646.253750	8.985805	-0.051577	4.711007
249.110204	7654.250975	8.990810	-0.051562	4.713397
249.191920	7662.247474	8.995815	-0.051583	4.715785
249.477235	7670.323004	9.000819	-0.051642	4.718194
249.828856	7678.249464	9.005824	-0.051712	4.720558
250.026427	7686.304377	9.010829	-0.051755	4.722959
250.109609	7694.331016	9.015834	-0.051776	4.725351
250.187305	7702.345984	9.020839	-0.051795	4.727738
250.452744	7710.366792	9.025843	-0.051850	4.730125
250.406267	7718.424477	9.030848	-0.051847	4.732522
250.755413	7726.429178	9.035853	-0.051917	4.734902
250.641928	7734.425062	9.040858	-0.051902	4.737279
250.790191	7742.398139	9.045863	-0.051935	4.739648
251.217287	7750.467527	9.050867	-0.052020	4.742042
251.393577	7758.412277	9.055872	-0.052058	4.744400
251.377708	7766.512694	9.060877	-0.052060	4.746803
251.414508	7774.505097	9.065882	-0.052073	4.749172
251.568580	7782.502811	9.070887	-0.052107	4.751542
251.986021	7790.568702	9.075891	-0.052190	4.753930
251.904506	7798.584575	9.080896	-0.052180	4.756303
251.913777	7806.523170	9.085901	-0.052187	4.758652
252.453599	7814.541674	9.090906	-0.052293	4.761022
252.440183	7822.532370	9.095911	-0.052296	4.763384
252.663022	7830.591230	9.100915	-0.052343	4.765764
252.894690	7838.597219	9.105920	-0.052392	4.768127
252.847036	7846.564603	9.110925	-0.052388	4.770479
252.747649	7854.686615	9.115930	-0.052375	4.772876
252.985805	7862.665628	9.120935	-0.052425	4.775227
253.404813	7870.710401	9.125939	-0.052508	4.777597
253.446527	7878.623881	9.130944	-0.052521	4.779928
253.496337	7886.664393	9.135949	-0.052536	4.782295
253.710702	7894.688902	9.140954	-0.052581	4.784655
253.784580	7902.701696	9.145959	-0.052601	4.787012
253.920498	7910.706608	9.150963	-0.052631	4.789364
253.903830	7918.728201	9.155968	-0.052634	4.791722
254.126440	7926.807208	9.160973	-0.052680	4.794093
254.190951	7934.809252	9.165978	-0.052698	4.796442
254.677364	7942.757705	9.170983	-0.052794	4.798772
254.778026	7950.820436	9.175987	-0.052818	4.801136
254.654243	7958.794248	9.180992	-0.052800	4.803474
254.808692	7966.789024	9.185997	-0.052834	4.805815
255.123045	7974.869199	9.191002	-0.052898	4.808180
255.089615	7982.836973	9.196007	-0.052898	4.810512
255.155762	7990.326652	9.201011	-0.052915	4.812703
255.395014	7994.878532	9.206016	-0.052963	4.814033
255.706847	7997.428287	9.211021	-0.053023	4.814777
255.600172	7998.717738	9.216026	-0.053004	4.815154
255.647969	7999.159630	9.221031	-0.053013	4.815283
256.043516	8000.209627	9.226035	-0.053088	4.815588
255.984296	8000.163814	9.231040	-0.053077	4.815575
255.901054	8000.192375	9.236045	-0.053062	4.815584
255.866598	8000.159784	9.241050	-0.053055	4.815574
255.894689	8000.153852	9.246055	-0.053061	4.815572
256.145232	8000.184671	9.251059	-0.053108	4.815580
256.256453	8000.170486	9.256064	-0.053128	4.815576
256.349579	8000.221161	9.261069	-0.053146	4.815590
256.234519	8000.186182	9.266074	-0.053125	4.815580
256.359883	8000.180774	9.271079	-0.053148	4.815578
256.454768	8000.185548	9.276083	-0.053166	4.815579
256.450906	8000.169479	9.281088	-0.053166	4.815574
256.573579	8000.169367	9.286093	-0.053189	4.815574
256.537933	8000.169869	9.291098	-0.053182	4.815574
256.663210	8000.181549	9.296103	-0.053206	4.815577
256.817981	8000.194781	9.301107	-0.053235	4.815580
256.720578	8000.167567	9.306112	-0.053217	4.815572
256.877524	8000.225696	9.311117	-0.053246	4.815589
256.750585	8000.193727	9.316122	-0.053223	4.815580
256.709857	8000.201622	9.321127	-0.053215	4.815582
256.952261	8000.207743	9.326131	-0.053261	4.815583
256.789612	8000.168780	9.331136	-0.053231	4.815572
256.867530	8000.201048	9.336141	-0.053245	4.815582
256.880980	8000.178854	9.341146	-0.053248	4.815575
257.248417	8000.188091	9.346151	-0.053317	4.815576
257.227176	8000.204850	9.351155	-0.053313	4.815581
257.249769	8000.227667	9.356160	-0.053317	4.815587
257.430370	8000.248800	9.361165	-0.053351	4.815593
257.282838	8000.239992	9.366170	-0.053324	4.815591
257.234160	8000.213576	9.371175	-0.053315	4.815583
257.494359	8000.240284	9.376179	-0.053363	4.815590
257.327624	8000.208730	9.381184	-0.053333	4.815582
257.315420	8000.248068	9.386189	-0.053331	4.815593
257.235902	8000.193375	9.391194	-0.053316	4.815577
257.288460	8000.187844	9.396199	-0.053326	4.815576
257.451854	8000.230057	9.401203	-0.053356	4.815587
257.424022	8000.191165	9.406208	-0.053351	4.815576
257.566706	8000.214881	9.411213	-0.053378	4.815582
257.400644	8000.207905	9.416218	-0.053348	4.815581
257.528549	8000.224971	9.421223	-0.053372	4.815585
257.521319	8000.250505	9.426227	-0.053370	4.815593
257.689783	8000.213758	9.431232	-0.053402	4.815581
257.658348	8000.216464	9.436237	-0.053396	4.815582
257.678014	8000.177281	9.441242	-0.053400	4.815571
257.719293	8000.220700	9.446247	-0.053408	4.815583
257.673767	8000.237062	9.451251	-0.053400	4.815588
257.463149	8000.205857	9.456256	-0.053361	4.815580
257.793634	8000.248671	9.461261	-0.053422	4.815591
257.797896	8000.231667	9.466266	-0.053423	4.815586
257.508429	8000.220534	9.471271	-0.053370	4.815584
257.481668	8000.227589	9.476275	-0.053365	4.815586
257.566291	8000.200151	9.481280	-0.053381	4.815578
257.611028	8000.236150	9.486285	-0.053389	4.815588
257.679189	8000.219124	9.491290	-0.053402	4.815583
257.645987	8000.210052	9.496295	-0.053396	4.815580
257.768895	8000.247330	9.501299	-0.053419	4.815591
257.628746	8000.179894	9.506304	-0.053393	4.815572
257.708931	8000.192973	9.511309	-0.053408	4.815575
257.808652	8000.193555	9.516314	-0.053427	4.815575
257.587207	8000.209172	9.521319	-0.053386	4.815580
257.709351	8000.195166	9.526323	-0.053409	4.815576
257.861578	8000.209426	9.531328	-0.053438	4.815579
257.702036	8000.218579	9.536333	-0.053408	4.815582
257.516772	8000.166426	9.541338	-0.053374	4.815568
257.686464	8000.198062	9.546343	-0.053406	4.815577
257.907218	8000.236944	9.551347	-0.053447	4.815587
257.937723	8000.215028	9.556352	-0.053453	4.815580
257.866146	8000.234168	9.561357	-0.053440	4.815586
257.838767	8000.230531	9.566362	-0.053435	4.815585
257.864137	8000.208532	9.571367	-0.053440	4.815579
257.862966	8000.194643	9.576371	-0.053440	4.815575
257.850795	8000.157075	9.581376	-0.053438	4.815564
257.971249	8000.214608	9.586381	-0.053460	4.815580
258.003576	8000.195927	9.591386	-0.053466	4.815574
258.000706	8000.195897	9.596391	-0.053466	4.815574
258.010557	8000.214234	9.601395	-0.053468	4.815580
257.923131	8000.195728	9.606400	-0.053452	4.815575
257.911238	8000.236140	9.611405	-0.053450	4.815587
257.994233	8000.239652	9.616410	-0.053466	4.815587
258.027436	8000.232735	9.621415	-0.053472	4.815585
258.005196	8000.258024	9.626419	-0.053468	4.815592
258.055610	8000.266343	9.631424	-0.053478	4.815595
257.856761	8000.278057	9.636429	-0.053441	4.815599
257.961736	8000.222112	9.641434	-0.053460	4.815582
258.149167	8000.223062	9.646439	-0.053496	4.815582
258.324151	8000.254786	9.651443	-0.053528	4.815590
258.144722	8000.234772	9.656448	-0.053495	4.815585
258.181173	8000.250341	9.661453	-0.053502	4.815589
258.376441	8000.242874	9.666458	-0.053539	4.815586
258.223448	8000.222225	9.671463	-0.053510	4.815581
258.246243	8000.254661	9.676467	-0.053515	4.815590
258.118643	8000.209860	9.681472	-0.053491	4.815578
258.165674	8000.234147	9.686477	-0.053500	4.815585
258.324206	8000.235692	9.691482	-0.053530	4.815584
258.280810	8000.220043	9.696487	-0.053522	4.815580
258.330183	8000.218732	9.701491	-0.053531	4.815579
258.128202	8000.182327	9.706496	-0.053494	4.815570
258.319024	8000.247423	9.711501	-0.053530	4.815588
258.628918	8000.222608	9.716506	-0.053588	4.815579
258.366610	8000.206577	9.721511	-0.053539	4.815576
258.296492	8000.242831	9.726515	-0.053526	4.815587
258.362063	8000.217218	9.731520	-0.053538	4.815579
258.573704	8000.247406	9.736525	-0.053578	4.815587
258.580089	8000.252868	9.741530	-0.053579	4.815588
258.303211	8000.245144	9.746535	-0.053528	4.815587
258.300510	8000.249389	9.751539	-0.053528	4.815588
258.305660	8000.225990	9.756544	-0.053529	4.815582
258.363952	8000.229098	9.761549	-0.053540	4.815582
258.557176	8000.251507	9.766554	-0.053576	4.815588
258.194885	8000.223157	9.771559	-0.053509	4.815581
258.151631	8000.211783	9.776563	-0.053501	4.815578
258.286691	8000.197989	9.781568	-0.053526	4.815573
258.453449	8000.237056	9.786573	-0.053557	4.815584
258.392759	8000.207237	9.791578	-0.053546	4.815576
258.486368	8000.217333	9.796583	-0.053564	4.815578
258.516794	8000.225325	9.801587	-0.053570	4.815580
258.367862	8000.227174	9.806592	-0.053542	4.815582
258.347260	8000.233263	9.811597	-0.053539	4.815583
258.362844	8000.222853	9.816602	-0.053542	4.815580
258.233888	8000.213279	9.821607	-0.053518	4.815578
258.428748	8000.254943	9.826611	-0.053554	4.815589
258.559879	8000.211176	9.831616	-0.053579	4.815576
258.514001	8000.238213	9.836621	-0.053571	4.815584
258.356192	8000.231372	9.841626	-0.053541	4.815583
258.323094	8000.244732	9.846631	-0.053535	4.815587
258.808073	8000.256968	9.851635	-0.053626	4.815588
259.311868	8000.222513	9.856640	-0.053720	4.815576
258.832073	8000.247781	9.861645	-0.053631	4.815585
258.838806	8000.243635	9.866650	-0.053632	4.815584
258.732365	8000.223748	9.871655	-0.053613	4.815579
258.679519	8000.303013	9.876659	-0.053603	4.815602
258.786721	8000.269536	9.881664	-0.053623	4.815592
258.895333	8000.252105	9.886669	-0.053644	4.815586
258.760977	8000.280897	9.891674	-0.053619	4.815595
258.666807	8000.258007	9.896679	-0.053601	4.815589
258.793769	8000.252626	9.901683	-0.053625	4.815587
258.621765	8000.237006	9.906688	-0.053593	4.815583
258.691647	8000.244577	9.911693	-0.053607	4.815585
258.896364	8000.254357	9.916698	-0.053645	4.815587
258.808815	8000.226234	9.921703	-0.053629	4.815579
258.756582	8000.249963	9.926707	-0.053619	4.815586
258.478615	8000.201630	9.931712	-0.053568	4.815573
258.519464	8000.240770	9.936717	-0.053575	4.815585
258.649880	8000.199128	9.941722	-0.053600	4.815572
258.831450	8000.205324	9.946727	-0.053634	4.815573
258.883770	8000.230767	9.951731	-0.053644	4.815580
258.543121	8000.194224	9.956736	-0.053581	4.815571
258.603984	8000.233692	9.961741	-0.053592	4.815582
258.748528	8000.235009	9.966746	-0.053619	4.815582
258.790274	8000.204732	9.971751	-0.053627	4.815573
258.810525	8000.223240	9.976755	-0.053631	4.815578
258.522487	8000.200378	9.981760	-0.053578	4.815573
258.703238	8000.231129	9.986765	-0.053612	4.815581
258.909243	8000.232385	9.991770	-0.053650	4.815580
258.796043	8000.234819	9.996775	-0.053629	4.815582
258.801882	8000.254159	10.001779	-0.053630	4.815587
258.770195	8000.253656	10.006784	-0.053625	4.815587
258.626798	8000.245982	10.011789	-0.053598	4.815586
258.771008	8000.275066	10.016794	-0.053625	4.815593
258.844045	8000.257052	10.021799	-0.053639	4.815588
258.913302	8000.263545	10.026803	-0.053652	4.815589
258.751687	8000.221390	10.031808	-0.053622	4.815578
258.837489	8000.246312	10.036813	-0.053638	4.815585
258.828613	8000.270752	10.041818	-0.053637	4.815592
258.639726	8000.205718	10.046823	-0.053602	4.815574
258.917458	8000.245536	10.051827	-0.053654	4.815584
258.835316	8000.199343	10.056832	-0.053639	4.815571
258.608740	8000.213806	10.061837	-0.053597	4.815576
258.761453	8000.208847	10.066842	-0.053625	4.815574
258.924705	8000.231835	10.071847	-0.053656	4.815580
258.977054	8000.226300	10.076851	-0.053666	4.815578
258.977720	8000.218850	10.081856	-0.053666	4.815576
258.759202	8000.221695	10.086861	-0.053626	4.815578
258.830281	8000.208990	10.091866	-0.053639	4.815574
258.842714	8000.223096	10.096871	-0.053642	4.815578
259.084522	8000.256985	10.101875	-0.053687	4.815587
258.839807	8000.244446	10.106880	-0.053641	4.815584
258.637171	8000.275324	10.111885	-0.053604	4.815594
258.669607	8000.255576	10.116890	-0.053610	4.815588
258.883029	8000.233454	10.121895	-0.053650	4.815581
258.781895	8000.231813	10.126899	-0.053631	4.815581
258.640436	8000.209216	10.131904	-0.053605	4.815575
258.788272	8000.220200	10.136909	-0.053633	4.815577
258.876672	8000.221665	10.141914	-0.053650	4.815577
258.782165	8000.220133	10.146919	-0.053632	4.815577
258.483050	8000.233408	10.151923	-0.053577	4.815582
258.520538	8000.199857	10.156928	-0.053584	4.815572
258.607082	8000.230132	10.161933	-0.053600	4.815581
258.712708	8000.235084	10.166938	-0.053620	4.815582
258.658904	8000.221401	10.171943	-0.053610	4.815578
258.750514	8000.233601	10.176947	-0.053627	4.815581
258.520024	8000.206340	10.181952	-0.053585	4.815574
258.907194	8000.258633	10.186957	-0.053657	4.815588
259.001885	8000.274088	10.191962	-0.053675	4.815592
258.564967	8000.212467	10.196967	-0.053594	4.815576
258.597803	8000.265363	10.201971	-0.053600	4.815591
258.487496	8000.249686	10.206976	-0.053580	4.815587
258.539804	8000.240946	10.211981	-0.053590	4.815584
258.809834	8000.250728	10.216986	-0.053640	4.815586
258.810324	8000.188797	10.221991	-0.053640	4.815568
258.677249	8000.241111	10.226995	-0.053616	4.815584
258.595971	8000.187455	10.232000	-0.053601	4.815568
258.637576	8000.242630	10.237005	-0.053609	4.815584
258.888310	8000.263847	10.242010	-0.053656	4.815589
258.679447	8000.232668	10.247015	-0.053617	4.815581
258.821561	8000.231808	10.252019	-0.053644	4.815580
258.820967	8000.262793	10.257024	-0.053644	4.815589
258.919463	8000.261219	10.262029	-0.053662	4.815588
258.765984	8000.252311	10.267034	-0.053634	4.815587
258.439467	8000.220273	10.272039	-0.053573	4.815579
258.955766	8000.273614	10.277043	-0.053669	4.815592
258.713385	8000.222658	10.282048	-0.053624	4.815578
258.831594	8000.255589	10.287053	-0.053647	4.815587
258.750515	8000.250004	10.292058	-0.053632	4.815586
258.474284	8000.207040	10.297063	-0.053581	4.815575
258.678047	8000.249918	10.302067	-0.053619	4.815586
259.016642	8000.213823	10.307072	-0.053682	4.815574
258.949204	8000.225553	10.312077	-0.053670	4.815578
258.863567	8000.242326	10.317082	-0.053654	4.815583
258.772492	8000.225895	10.322087	-0.053637	4.815579
259.030629	8000.295302	10.327091	-0.053685	4.815598
258.841626	8000.278335	10.332096	-0.053650	4.815594
258.773272	8000.252662	10.337101	-0.053638	4.815587
258.886581	8000.255604	10.342106	-0.053659	4.815587
258.884440	8000.226744	10.347111	-0.053659	4.815578
258.954828	8000.269574	10.352115	-0.053672	4.815591
258.824263	8000.233269	10.357120	-0.053648	4.815581
258.797071	8000.243521	10.362125	-0.053643	4.815584
258.604196	8000.240377	10.367130	-0.053607	4.815584
258.670189	8000.206225	10.372135	-0.053620	4.815573
258.813999	8000.244917	10.377139	-0.053647	4.815584
258.715372	8000.230499	10.382144	-0.053629	4.815580
258.786662	8000.255184	10.387149	-0.053642	4.815587
258.920606	8000.230690	10.392154	-0.053667	4.815579
258.710340	8000.218716	10.397159	-0.053628	4.815577
258.860994	8000.217996	10.402163	-0.053656	4.815576
258.890226	8000.207810	10.407168	-0.053662	4.815573
258.843196	8000.234829	10.412173	-0.053654	4.815581
258.592298	8000.207234	10.417178	-0.053607	4.815574
258.896496	8000.222917	10.422183	-0.053664	4.815577
258.908072	8000.257306	10.427187	-0.053666	4.815587
258.658221	8000.207296	10.432192	-0.053620	4.815574
258.734552	8000.221381	10.437197	-0.053634	4.815577
259.059176	8000.239536	10.442202	-0.053695	4.815581
258.894087	8000.186642	10.447207	-0.053664	4.815567
258.658380	8000.227660	10.452211	-0.053621	4.815580
258.726930	8000.211709	10.457216	-0.053634	4.815575
258.647105	8000.222168	10.462221	-0.053619	4.815578
258.798796	8000.291966	10.467226	-0.053647	4.815598
258.695214	8000.263580	10.472231	-0.053628	4.815590
258.735165	8000.267456	10.477235	-0.053636	4.815591
258.911956	8000.261824	10.482240	-0.053669	4.815588
258.851764	8000.239491	10.487245	-0.053658	4.815582
258.977490	8000.235158	10.492250	-0.053682	4.815580
258.847023	8000.200991	10.497255	-0.053657	4.815571
258.977644	8000.257626	10.502259	-0.053682	4.815587
258.796456	8000.201264	10.507264	-0.053648	4.815571
258.915349	8000.233138	10.512269	-0.053671	4.815580
258.976714	8000.256592	10.517274	-0.053682	4.815587
258.688137	8000.223039	10.522279	-0.053629	4.815578
259.137772	8000.258197	10.527283	-0.053713	4.815586
258.804246	8000.245270	10.532288	-0.053651	4.815584
258.737119	8000.243118	10.537293	-0.053639	4.815584
259.060470	8000.280480	10.542298	-0.053699	4.815593
258.995315	8000.238837	10.547303	-0.053687	4.815581
258.974377	8000.273761	10.552307	-0.053683	4.815592
258.921527	8000.264366	10.557312	-0.053674	4.815589
258.951534	8000.264874	10.562317	-0.053679	4.815589
258.946422	8000.291512	10.567322	-0.053679	4.815597
259.018707	8000.241440	10.572327	-0.053692	4.815582
259.038276	8000.230027	10.577331	-0.053696	4.815578
258.984536	8000.243049	10.582336	-0.053686	4.815582
258.852961	8000.218477	10.587341	-0.053662	4.815576
258.948856	8000.196565	10.592346	-0.053680	4.815569
259.018772	8000.216955	10.597351	-0.053693	4.815575
258.993369	8000.255010	10.602355	-0.053689	4.815586
258.802458	8000.207034	10.607360	-0.053653	4.815573
259.079576	8000.235092	10.612365	-0.053705	4.815580
258.883920	8000.232971	10.617370	-0.053669	4.815580
258.879717	8000.224373	10.622375	-0.053668	4.815577
259.144684	8000.251164	10.627379	-0.053718	4.815584
258.946082	8000.244721	10.632384	-0.053681	4.815583
259.073205	8000.275662	10.637389	-0.053705	4.815592
259.282806	8000.289797	10.642394	-0.053744	4.815595
259.011590	8000.258663	10.647399	-0.053694	4.815587
259.152167	8000.285552	10.652403	-0.053720	4.815594
259.065650	8000.269195	10.657408	-0.053704	4.815590
259.144959	8000.255557	10.662413	-0.053719	4.815585
259.002011	8000.306641	10.667418	-0.053693	4.815601
259.111642	8000.312727	10.672423	-0.053713	4.815602
259.265316	8000.294967	10.677427	-0.053742	4.815596
259.087440	8000.302750	10.682432	-0.053709	4.815599
258.959323	8000.278234	10.687437	-0.053686	4.815593
258.998585	8000.321622	10.692442	-0.053693	4.815605
259.041567	8000.267865	10.697447	-0.053701	4.815589
258.903424	8000.263481	10.702451	-0.053676	4.815589
258.970836	8000.243238	10.707456	-0.053688	4.815582
259.104833	8000.263611	10.712461	-0.053714	4.815588
259.331706	8000.290846	10.717466	-0.053756	4.815595
259.128321	8000.251210	10.722471	-0.053718	4.815584
258.964472	8000.278451	10.727475	-0.053688	4.815593
259.048309	8000.280910	10.732480	-0.053704	4.815593
258.969296	8000.253995	10.737485	-0.053689	4.815586
259.079484	8000.302818	10.742490	-0.053710	4.815599
259.146777	8000.241982	10.747495	-0.053723	4.815581
259.181087	8000.285289	10.752499	-0.053729	4.815594
258.942723	8000.247216	10.757504	-0.053685	4.815584
258.931960	8000.256670	10.762509	-0.053683	4.815587
259.280191	8000.281622	10.767514	-0.053748	4.815592
259.155464	8000.239002	10.772519	-0.053725	4.815580
259.051437	8000.285383	10.777523	-0.053706	4.815594
259.145843	8000.262378	10.782528	-0.053724	4.815587
259.261136	8000.245057	10.787533	-0.053745	4.815582
259.071123	8000.277210	10.792538	-0.053710	4.815592
259.038692	8000.279899	10.797543	-0.053704	4.815593
259.090364	8000.265808	10.802547	-0.053714	4.815588
259.112437	8000.265118	10.807552	-0.053719	4.815588
259.150842	8000.283924	10.812557	-0.053726	4.815593
259.138009	8000.330731	10.817562	-0.053724	4.815607
259.010330	8000.248539	10.822567	-0.053700	4.815584
259.095193	8000.264902	10.827571	-0.053716	4.815588
259.084254	8000.294649	10.832576	-0.053714	4.815597
259.220549	8000.264853	10.837581	-0.053740	4.815587
259.214278	8000.323518	10.842586	-0.053739	4.815605
259.158329	8000.263866	10.847591	-0.053729	4.815587
259.104143	8000.269404	10.852595	-0.053719	4.815589
259.096381	8000.214815	10.857600	-0.053717	4.815573
259.107979	8000.220362	10.862605	-0.053720	4.815575
259.261276	8000.235710	10.867610	-0.053749	4.815579
259.052761	8000.224832	10.872615	-0.053710	4.815577
259.075650	8000.282906	10.877619	-0.053714	4.815593
259.096136	8000.256554	10.882624	-0.053718	4.815586
259.147479	8000.254207	10.887629	-0.053728	4.815585
259.411884	8000.269240	10.892634	-0.053778	4.815588
259.107799	8000.257863	10.897639	-0.053721	4.815586
259.058796	8000.294463	10.902643	-0.053712	4.815597
259.185813	8000.265584	10.907648	-0.053736	4.815588
259.255153	8000.248577	10.912653	-0.053749	4.815582
259.236322	8000.287809	10.917658	-0.053746	4.815594
259.125124	8000.339413	10.922663	-0.053725	4.815610
259.251356	8000.295566	10.927667	-0.053749	4.815596
259.279001	8000.237284	10.932672	-0.053754	4.815579
259.382707	8000.251819	10.937677	-0.053774	4.815583
259.222113	8000.269499	10.942682	-0.053744	4.815589
259.104456	8000.228064	10.947687	-0.053722	4.815577
259.534276	8000.288536	10.952691	-0.053803	4.815593
259.392746	8000.278755	10.957696	-0.053776	4.815591
259.128921	8000.254151	10.962701	-0.053727	4.815585
259.347733	8000.346416	10.967706	-0.053768	4.815611
259.297252	8000.266557	10.972711	-0.053759	4.815587
259.186387	8000.305349	10.977715	-0.053739	4.815599
259.349440	8000.272787	10.982720	-0.053769	4.815589
259.276789	8000.261999	10.987725	-0.053756	4.815586
259.402744	8000.259807	10.992730	-0.053780	4.815585
259.192051	8000.235006	10.997735	-0.053741	4.815579
259.240785	8000.274277	11.002739	-0.053750	4.815590
259.164118	8000.265559	11.007744	-0.053736	4.815588
259.098406	8000.263430	11.012749	-0.053724	4.815587
259.311382	8000.263733	11.017754	-0.053764	4.815587
259.309354	8000.225261	11.022759	-0.053763	4.815575
259.244536	8000.259466	11.027763	-0.053751	4.815586
259.234664	8000.253980	11.032768	-0.053750	4.815584
259.210421	8000.237576	11.037773	-0.053745	4.815579
259.270285	8000.270620	11.042778	-0.053757	4.815589
259.257935	8000.231978	11.047783	-0.053755	4.815577
259.275712	8000.268606	11.052787	-0.053758	4.815588
259.220527	8000.245285	11.057792	-0.053748	4.815582
259.225576	8000.243248	11.062797	-0.053749	4.815581
259.392929	8000.284463	11.067802	-0.053781	4.815592
259.174440	8000.271285	11.072807	-0.053740	4.815589
259.283382	8000.286974	11.077811	-0.053761	4.815593
259.259895	8000.286605	11.082816	-0.053756	4.815593
259.251063	8000.268317	11.087821	-0.053755	4.815588
259.292503	8000.288241	11.092826	-0.053763	4.815594
259.367513	8000.253168	11.097831	-0.053777	4.815583
259.339460	8000.277294	11.102835	-0.053772	4.815590
259.508636	8000.261924	11.107840	-0.053804	4.815585
259.017883	8000.229327	11.112845	-0.053712	4.815578
259.394190	8000.264354	11.117850	-0.053783	4.815586
259.253723	8000.242840	11.122855	-0.053757	4.815581
259.306925	8000.270434	11.127859	-0.053767	4.815588
259.336670	8000.248505	11.132864	-0.053773	4.815582
259.470637	8000.247513	11.137869	-0.053798	4.815581
259.537136	8000.271053	11.142874	-0.053810	4.815587
259.388926	8000.253685	11.147879	-0.053783	4.815583
259.585646	8000.280427	11.152883	-0.053820	4.815590
259.619860	8000.261776	11.157888	-0.053826	4.815584
259.400080	8000.243235	11.162893	-0.053785	4.815580
259.494856	8000.271511	11.167898	-0.053803	4.815588
259.455595	8000.256997	11.172903	-0.053796	4.815584
259.391253	8000.282664	11.177907	-0.053784	4.815592
259.448695	8000.259053	11.182912	-0.053795	4.815584
259.329777	8000.241097	11.187917	-0.053773	4.815580
259.511400	8000.262251	11.192922	-0.053807	4.815585
259.396156	8000.264651	11.197927	-0.053786	4.815586
259.535528	8000.276566	11.202931	-0.053812	4.815589
259.534166	8000.257332	11.207936	-0.053812	4.815583
259.308301	8000.225873	11.212941	-0.053770	4.815575
259.330606	8000.286075	11.217946	-0.053775	4.815593
259.616518	8000.249118	11.222951	-0.053828	4.815581
259.609670	8000.292819	11.227955	-0.053827	4.815593
259.519774	8000.239020	11.232960	-0.053810	4.815578
259.459735	8000.240188	11.237965	-0.053799	4.815579
259.551548	8000.254529	11.242970	-0.053817	4.815582
259.592883	8000.237063	11.247975	-0.053825	4.815577
259.516478	8000.273215	11.252979	-0.053811	4.815588
259.469179	8000.272456	11.257984	-0.053802	4.815588
259.315306	8000.248586	11.262989	-0.053773	4.815582
259.560621	8000.276125	11.267994	-0.053819	4.815589
259.534305	8000.245800	11.272999	-0.053815	4.815580
259.560921	8000.271890	11.278003	-0.053820	4.815587
259.325124	8000.256290	11.283008	-0.053776	4.815584
259.352567	8000.248211	11.288013	-0.053781	4.815582
259.356115	8000.255763	11.293018	-0.053782	4.815584
259.396668	8000.252172	11.298023	-0.053790	4.815582
259.494293	8000.252720	11.303027	-0.053808	4.815582
259.499394	8000.228252	11.308032	-0.053809	4.815575
259.323966	8000.232870	11.313037	-0.053777	4.815577
259.378665	8000.251943	11.318042	-0.053787	4.815582
259.488291	8000.214233	11.323047	-0.053808	4.815571
259.548979	8000.244086	11.328051	-0.053819	4.815579
259.351455	8000.236592	11.333056	-0.053783	4.815578
259.362211	8000.235716	11.338061	-0.053785	4.815578
259.653142	8000.284299	11.343066	-0.053839	4.815591
259.500482	8000.243357	11.348071	-0.053811	4.815579
259.578841	8000.269227	11.353075	-0.053826	4.815587
259.677357	8000.254836	11.358080	-0.053844	4.815582
259.320657	8000.245800	11.363085	-0.053778	4.815581
259.388706	8000.305684	11.368090	-0.053791	4.815598
259.446462	8000.252168	11.373095	-0.053802	4.815582
259.666853	8000.275026	11.378099	-0.053843	4.815588
259.602926	8000.279335	11.383104	-0.053832	4.815589
259.406162	8000.241943	11.388109	-0.053795	4.815579
259.667520	8000.281496	11.393114	-0.053844	4.815590
259.537498	8000.239857	11.398119	-0.053820	4.815578
259.473421	8000.294370	11.403123	-0.053808	4.815594
259.706027	8000.315292	11.408128	-0.053852	4.815599
259.531496	8000.257968	11.413133	-0.053819	4.815583
259.450317	8000.266267	11.418138	-0.053804	4.815586
259.559427	8000.248845	11.423143	-0.053825	4.815581
259.581702	8000.302637	11.428147	-0.053829	4.815596
259.402737	8000.284765	11.433152	-0.053796	4.815592
259.268804	8000.237721	11.438157	-0.053771	4.815579
259.406532	8000.277383	11.443162	-0.053797	4.815590
259.413018	8000.261482	11.448167	-0.053799	4.815585
259.533542	8000.261338	11.453171	-0.053821	4.815584
259.439115	8000.267284	11.458176	-0.053804	4.815587
259.310930	8000.269472	11.463181	-0.053780	4.815588
259.404341	8000.276361	11.468186	-0.053798	4.815589
259.433580	8000.249084	11.473191	-0.053803	4.815581
259.693188	8000.280062	11.478195	-0.053852	4.815589
259.687586	8000.334466	11.483200	-0.053851	4.815605
259.651165	8000.286883	11.488205	-0.053844	4.815591
259.597151	8000.318061	11.493210	-0.053835	4.815601
259.555952	8000.310993	11.498215	-0.053827	4.815599
259.453126	8000.291164	11.503219	-0.053808	4.815593
259.502848	8000.332588	11.508224	-0.053818	4.815605
259.504371	8000.267468	11.513229	-0.053818	4.815586
259.443258	8000.298529	11.518234	-0.053807	4.815596
259.559677	8000.273749	11.523239	-0.053829	4.815588
259.664738	8000.297921	11.528243	-0.053849	4.815594
259.641775	8000.282606	11.533248	-0.053844	4.815590
259.536467	8000.253122	11.538253	-0.053825	4.815582
259.743617	8000.301400	11.543258	-0.053864	4.815595
259.687740	8000.318660	11.548263	-0.053854	4.815600
259.660701	8000.277641	11.553267	-0.053849	4.815588
259.763176	8000.269724	11.558272	-0.053868	4.815586
259.791054	8000.242423	11.563277	-0.053873	4.815577
259.748581	8000.284473	11.568282	-0.053866	4.815590
259.806522	8000.268348	11.573287	-0.053877	4.815585
259.813794	8000.282370	11.578291	-0.053878	4.815589
259.774746	8000.266792	11.583296	-0.053871	4.815585
259.630862	8000.233471	11.588301	-0.053844	4.815576
259.731256	8000.281067	11.593306	-0.053863	4.815589
259.802066	8000.263016	11.598311	-0.053877	4.815583
259.648022	8000.265848	11.603315	-0.053848	4.815585
259.623012	8000.288956	11.608320	-0.053844	4.815592
259.778011	8000.266944	11.613325	-0.053873	4.815585
259.575675	8000.294622	11.618330	-0.053835	4.815594
259.696405	8000.280595	11.623335	-0.053858	4.815589
259.739192	8000.297336	11.628339	-0.053866	4.815594
259.755685	8000.341421	11.633344	-0.053869	4.815606
259.604855	8000.271666	11.638349	-0.053841	4.815587
259.663840	8000.301492	11.643354	-0.053853	4.815595
259.721679	8000.291774	11.648359	-0.053864	4.815592
259.777370	8000.296977	11.653363	-0.053874	4.815593
259.927778	8000.299460	11.658368	-0.053902	4.815593
259.768194	8000.268017	11.663373	-0.053873	4.815585
259.799545	8000.303799	11.668378	-0.053879	4.815595
259.659755	8000.290842	11.673383	-0.053853	4.815592
259.732268	8000.280297	11.678387	-0.053867	4.815589
259.795538	8000.261054	11.683392	-0.053879	4.815583
259.616876	8000.261346	11.688397	-0.053846	4.815584
259.872161	8000.292254	11.693402	-0.053893	4.815592
259.676006	8000.275168	11.698407	-0.053857	4.815587
259.572780	8000.302334	11.703411	-0.053838	4.815596
259.731642	8000.262226	11.708416	-0.053868	4.815583
259.987031	8000.225837	11.713421	-0.053915	4.815572
260.038658	8000.291863	11.718426	-0.053925	4.815591
259.749408	8000.218770	11.723431	-0.053872	4.815571
259.804032	8000.259206	11.728435	-0.053882	4.815582
259.906814	8000.230998	11.733440	-0.053901	4.815573
259.759989	8000.237153	11.738445	-0.053874	4.815576
259.936937	8000.283868	11.743450	-0.053907	4.815589
259.952820	8000.247825	11.748455	-0.053910	4.815578
259.868231	8000.264615	11.753459	-0.053895	4.815583
259.923724	8000.266609	11.758464	-0.053905	4.815584
260.040768	8000.242907	11.763469	-0.053927	4.815576
259.906611	8000.267430	11.768474	-0.053903	4.815584
259.944113	8000.229605	11.773479	-0.053910	4.815573
259.935985	8000.264740	11.778483	-0.053908	4.815583
260.030553	8000.278058	11.783488	-0.053926	4.815587
259.725727	8000.253848	11.788493	-0.053870	4.815581
259.726947	8000.252816	11.793498	-0.053870	4.815581
259.777530	8000.242980	11.798503	-0.053880	4.815577
259.853882	8000.243180	11.803507	-0.053894	4.815577
259.796639	8000.261486	11.808512	-0.053884	4.815583
259.817163	8000.239407	11.813517	-0.053888	4.815576
259.919668	8000.290243	11.818522	-0.053907	4.815591
259.933926	8000.231740	11.823527	-0.053910	4.815573
259.971631	8000.240921	11.828531	-0.053917	4.815576
260.030781	8000.268613	11.833536	-0.053928	4.815584
259.734461	8000.276590	11.838541	-0.053873	4.815587
259.745977	8000.320592	11.843546	-0.053876	4.815600
259.825878	8000.325124	11.848551	-0.053891	4.815601
259.760910	8000.289892	11.853555	-0.053879	4.815591
259.713299	8000.258149	11.858560	-0.053870	4.815582
259.735870	8000.212602	11.863565	-0.053874	4.815569
259.869164	8000.269284	11.868570	-0.053899	4.815585
259.806153	8000.258653	11.873575	-0.053888	4.815582
259.647314	8000.261406	11.878579	-0.053858	4.815583
259.884202	8000.294149	11.883584	-0.053903	4.815592
259.643053	8000.295553	11.888589	-0.053858	4.815593
259.772589	8000.295557	11.893594	-0.053882	4.815593
259.786129	8000.232770	11.898599	-0.053885	4.815574
259.734323	8000.261848	11.903603	-0.053876	4.815583
259.758342	8000.251576	11.908608	-0.053880	4.815580
259.792282	8000.221170	11.913613	-0.053887	4.815571
260.191216	8000.266185	11.918618	-0.053961	4.815582
259.929772	8000.302507	11.923623	-0.053913	4.815594
259.795240	8000.276816	11.928627	-0.053888	4.815587
260.096268	8000.292451	11.933632	-0.053944	4.815590
259.865935	8000.250235	11.938637	-0.053901	4.815579
259.862373	8000.298263	11.943642	-0.053901	4.815593
259.949021	8000.253766	11.948647	-0.053917	4.815580
260.078759	8000.270866	11.953651	-0.053942	4.815584
259.803884	8000.282398	11.958656	-0.053891	4.815589
259.684217	8000.231315	11.963661	-0.053868	4.815574
260.084718	8000.262467	11.968666	-0.053943	4.815582
260.122745	8000.247084	11.973671	-0.053951	4.815577
260.116200	8000.264085	11.978675	-0.053949	4.815582
260.297471	8000.288439	11.983680	-0.053983	4.815588
260.110018	8000.277904	11.988685	-0.053949	4.815586
260.055536	8000.278095	11.993690	-0.053939	4.815586
259.910586	8000.242620	11.998695	-0.053912	4.815577
260.060151	8000.261112	12.003699	-0.053940	4.815581
260.067775	8000.264458	12.008704	-0.053942	4.815582
259.723339	8000.247077	12.013709	-0.053878	4.815579
260.014132	8000.305273	12.018714	-0.053932	4.815594
260.085481	8000.282958	12.023719	-0.053945	4.815587
259.905169	8000.268268	12.028723	-0.053912	4.815584
259.931512	8000.290081	12.033728	-0.053917	4.815590
260.018845	8000.266960	12.038733	-0.053934	4.815583
259.883662	8000.262624	12.043738	-0.053909	4.815582
260.059552	8000.260183	12.048743	-0.053942	4.815581
260.220180	8000.261766	12.053747	-0.053972	4.815581
260.076756	8000.276522	12.058752	-0.053945	4.815586
260.085394	8000.267066	12.063757	-0.053947	4.815583
260.177196	8000.322000	12.068762	-0.053964	4.815598
260.244189	8000.301750	12.073767	-0.053977	4.815592
260.223572	8000.289678	12.078771	-0.053973	4.815589
260.111881	8000.295341	12.083776	-0.053953	4.815591
260.056752	8000.263474	12.088781	-0.053943	4.815582
260.057875	8000.305171	12.093786	-0.053943	4.815594
260.185450	8000.251731	12.098791	-0.053967	4.815578
260.072980	8000.247767	12.103795	-0.053946	4.815577
260.125879	8000.272152	12.108800	-0.053956	4.815584
259.774336	8000.249312	12.113805	-0.053891	4.815579
260.023525	8000.277984	12.118810	-0.053938	4.815586
260.160639	8000.253543	12.123815	-0.053963	4.815578
260.261973	8000.264836	12.128819	-0.053982	4.815581
260.319022	8000.286085	12.133824	-0.053993	4.815587
260.210209	8000.270430	12.138829	-0.053973	4.815583
260.259077	8000.301158	12.143834	-0.053982	4.815592
260.209663	8000.290750	12.148839	-0.053973	4.815589
260.250033	8000.264723	12.153843	-0.053981	4.815581
260.392076	8000.336505	12.158848	-0.054008	4.815601
260.183744	8000.295716	12.163853	-0.053969	4.815591
260.217280	8000.320852	12.168858	-0.053975	4.815598
260.332719	8000.314216	12.173863	-0.053997	4.815595
260.208785	8000.276948	12.178867	-0.053974	4.815585
260.276823	8000.325083	12.183872	-0.053987	4.815599
260.154664	8000.304936	12.188877	-0.053965	4.815593
260.083745	8000.315540	12.193882	-0.053952	4.815597
260.030289	8000.292247	12.198887	-0.053942	4.815590
260.079742	8000.290938	12.203891	-0.053951	4.815590
260.376818	8000.342830	12.208896	-0.054007	4.815603
260.190431	8000.267149	12.213901	-0.053972	4.815582
260.248884	8000.291626	12.218906	-0.053983	4.815589
260.246602	8000.236056	12.223911	-0.053983	4.815573
260.186982	8000.282097	12.228915	-0.053972	4.815587
260.148908	8000.415020	12.233920	-0.053965	4.815626
260.168596	8000.302126	12.238925	-0.053969	4.815592
260.184547	8000.314154	12.243930	-0.053972	4.815596
260.061890	8000.331388	12.248935	-0.053950	4.815601
260.080022	8000.303927	12.253939	-0.053953	4.815593
260.185513	8000.309947	12.258944	-0.053973	4.815595
260.024590	8000.309461	12.263949	-0.053943	4.815595
260.232118	8000.347065	12.268954	-0.053982	4.815605
260.219750	8000.306285	12.273959	-0.053980	4.815593
260.058782	8000.311140	12.278963	-0.053950	4.815596
260.274030	8000.306140	12.283968	-0.053990	4.815593
260.323363	8000.279192	12.288973	-0.054000	4.815585
260.289244	8000.314969	12.293978	-0.053994	4.815596
260.162568	8000.290475	12.298983	-0.053970	4.815589
260.173664	8000.319516	12.303987	-0.053972	4.815597
260.426277	8000.372815	12.308992	-0.054020	4.815612
260.300383	8000.289580	12.313997	-0.053996	4.815588
260.189679	8000.297395	12.319002	-0.053976	4.815591
260.193841	8000.301753	12.324007	-0.053977	4.815592
260.104577	8000.284282	12.329011	-0.053961	4.815587
260.134139	8000.322172	12.334016	-0.053966	4.815598
260.374345	8000.297286	12.339021	-0.054011	4.815590
260.423136	8000.298102	12.344026	-0.054020	4.815590
260.322832	8000.313566	12.349031	-0.054002	4.815595
260.400259	8000.283873	12.354035	-0.054016	4.815586
260.519694	8000.295463	12.359040	-0.054039	4.815589
260.169892	8000.291879	12.364045	-0.053974	4.815589
260.389875	8000.296571	12.369050	-0.054015	4.815590
260.344345	8000.291568	12.374055	-0.054007	4.815588
260.195955	8000.288083	12.379059	-0.053979	4.815588
260.251437	8000.293282	12.384064	-0.053990	4.815589
260.260456	8000.272082	12.389069	-0.053992	4.815583
260.387335	8000.297681	12.394074	-0.054016	4.815590
260.248841	8000.296494	12.399079	-0.053990	4.815590
260.209082	8000.289449	12.404083	-0.053983	4.815588
260.337525	8000.302255	12.409088	-0.054007	4.815592
260.319618	8000.294500	12.414093	-0.054004	4.815589
260.510578	8000.312604	12.419098	-0.054040	4.815594
260.449555	8000.295596	12.424103	-0.054028	4.815589
260.230415	8000.281336	12.429107	-0.053988	4.815586
260.302831	8000.283608	12.434112	-0.054001	4.815586
260.388278	8000.267935	12.439117	-0.054017	4.815581
260.468070	8000.288488	12.444122	-0.054033	4.815587
260.508844	8000.296651	12.449127	-0.054040	4.815589
260.208505	8000.292810	12.454131	-0.053985	4.815589
260.464583	8000.314119	12.459136	-0.054032	4.815594
260.179427	8000.253910	12.464141	-0.053979	4.815578
260.478236	8000.334673	12.469146	-0.054035	4.815600
260.562411	8000.308295	12.474151	-0.054051	4.815592
260.450670	8000.282978	12.479155	-0.054031	4.815585
260.294788	8000.271892	12.484160	-0.054002	4.815583
260.384456	8000.240263	12.489165	-0.054019	4.815573
260.528895	8000.278969	12.494170	-0.054046	4.815584
260.545388	8000.345488	12.499175	-0.054049	4.815603
260.361401	8000.317917	12.504179	-0.054015	4.815596
260.611281	8000.335919	12.509184	-0.054062	4.815600
260.373220	8000.286096	12.514189	-0.054017	4.815587
260.524806	8000.303555	12.519194	-0.054046	4.815591
260.474655	8000.316636	12.524199	-0.054037	4.815595
260.477353	8000.334857	12.529203	-0.054037	4.815600
260.618499	8000.393807	12.534208	-0.054064	4.815617
260.351493	8000.260185	12.539213	-0.054014	4.815579
260.318508	8000.316277	12.544218	-0.054008	4.815596
260.452325	8000.298192	12.549223	-0.054034	4.815590
260.434527	8000.296849	12.554227	-0.054030	4.815589
260.646243	8000.320635	12.559232	-0.054070	4.815595
260.534427	8000.279292	12.564237	-0.054049	4.815584
260.344774	8000.313586	12.569242	-0.054014	4.815595
260.602671	8000.331721	12.574247	-0.054062	4.815599
260.560135	8000.302197	12.579251	-0.054055	4.815590
260.570143	8000.350449	12.584256	-0.054057	4.815604
260.477473	8000.325444	12.589261	-0.054040	4.815597
260.528868	8000.330576	12.594266	-0.054050	4.815599
260.637593	8000.348400	12.599271	-0.054070	4.815603
260.360270	8000.318229	12.604275	-0.054018	4.815596
260.570691	8000.300333	12.609280	-0.054058	4.815590
260.447876	8000.295130	12.614285	-0.054035	4.815589
260.463651	8000.312497	12.619290	-0.054038	4.815594
260.603273	8000.320145	12.624295	-0.054064	4.815595
260.574906	8000.299400	12.629299	-0.054059	4.815589
260.598738	8000.327582	12.634304	-0.054064	4.815597
260.564450	8000.284306	12.639309	-0.054058	4.815585
260.741691	8000.337438	12.644314	-0.054091	4.815600
260.747466	8000.337549	12.649319	-0.054092	4.815600
260.570664	8000.293004	12.654323	-0.054060	4.815587
260.872500	8000.339634	12.659328	-0.054116	4.815600
260.492096	8000.329137	12.664333	-0.054045	4.815598
260.687267	8000.356925	12.669338	-0.054082	4.815606
260.659633	8000.358625	12.674343	-0.054077	4.815606
260.463707	8000.283854	12.679347	-0.054041	4.815585
260.580624	8000.333860	12.684352	-0.054063	4.815599
260.422448	8000.297098	12.689357	-0.054033	4.815589
260.720655	8000.318030	12.694362	-0.054089	4.815594
260.489098	8000.363388	12.699367	-0.054046	4.815608
260.581580	8000.328601	12.704371	-0.054063	4.815598
260.756867	8000.341107	12.709376	-0.054096	4.815601
260.711116	8000.301916	12.714381	-0.054088	4.815589
260.729264	8000.315049	12.719386	-0.054092	4.815593
260.617916	8000.342082	12.724391	-0.054071	4.815601
260.636086	8000.296462	12.729395	-0.054075	4.815588
260.671104	8000.309872	12.734400	-0.054081	4.815592
260.564173	8000.295315	12.739405	-0.054062	4.815588
260.711014	8000.328720	12.744410	-0.054089	4.815597
260.673425	8000.277912	12.749415	-0.054082	4.815582
260.372312	8000.270853	12.754419	-0.054026	4.815582
260.551150	8000.294100	12.759424	-0.054060	4.815588
260.479330	8000.285460	12.764429	-0.054047	4.815586
260.517492	8000.306400	12.769434	-0.054054	4.815592
260.686204	8000.288887	12.774439	-0.054086	4.815586
260.639454	8000.265703	12.779443	-0.054077	4.815579
260.576125	8000.301002	12.784448	-0.054065	4.815590
260.552403	8000.330540	12.789453	-0.054061	4.815598
260.604164	8000.305768	12.794458	-0.054071	4.815591
260.607896	8000.320801	12.799463	-0.054072	4.815595
260.583492	8000.275551	12.804467	-0.054068	4.815582
260.684208	8000.291107	12.809472	-0.054086	4.815586
260.438736	8000.277482	12.814477	-0.054041	4.815583
260.542465	8000.300566	12.819482	-0.054060	4.815590
260.679624	8000.285740	12.824487	-0.054086	4.815585
260.807435	8000.262215	12.829491	-0.054110	4.815577
260.831435	8000.317107	12.834496	-0.054115	4.815593
260.661576	8000.317541	12.839501	-0.054083	4.815594
260.777579	8000.314120	12.844506	-0.054105	4.815592
260.773770	8000.305528	12.849511	-0.054105	4.815590
260.418609	8000.313605	12.854515	-0.054039	4.815594
260.719521	8000.339923	12.859520	-0.054095	4.815600
260.606347	8000.357312	12.864525	-0.054074	4.815606
260.550140	8000.304062	12.869530	-0.054064	4.815591
260.529411	8000.301602	12.874535	-0.054060	4.815590
260.617268	8000.278490	12.879539	-0.054077	4.815583
260.687596	8000.278592	12.884544	-0.054090	4.815582
260.730622	8000.271836	12.889549	-0.054098	4.815580
260.801935	8000.320026	12.894554	-0.054112	4.815594
260.643163	8000.288595	12.899559	-0.054082	4.815586
260.420131	8000.278544	12.904563	-0.054041	4.815584
260.503172	8000.299151	12.909568	-0.054057	4.815589
260.673927	8000.296627	12.914573	-0.054089	4.815588
260.728813	8000.307159	12.919578	-0.054099	4.815591
260.590607	8000.313454	12.924583	-0.054073	4.815593
260.691712	8000.292696	12.929587	-0.054092	4.815587
260.549617	8000.324566	12.934592	-0.054066	4.815596
260.607987	8000.297765	12.939597	-0.054077	4.815588
260.611618	8000.304251	12.944602	-0.054078	4.815590
260.635068	8000.276877	12.949607	-0.054083	4.815582
260.733669	8000.260351	12.954611	-0.054101	4.815577
260.558903	8000.292753	12.959616	-0.054069	4.815587
260.540746	8000.266834	12.964621	-0.054066	4.815580
260.583978	8000.291061	12.969626	-0.054074	4.815587
260.672520	8000.289325	12.974631	-0.054091	4.815586
260.747043	8000.280950	12.979635	-0.054105	4.815583
260.810960	8000.308722	12.984640	-0.054117	4.815591
260.550294	8000.257459	12.989645	-0.054068	4.815577
260.562925	8000.274775	12.994650	-0.054071	4.815582
260.794505	8000.266839	12.999655	-0.054114	4.815578
260.626666	8000.251284	13.004659	-0.054083	4.815575
260.876206	8000.276759	13.009664	-0.054130	4.815581
260.838947	8000.266550	13.014669	-0.054123	4.815578
260.860096	8000.282937	13.019674	-0.054127	4.815583
260.637480	8000.296394	13.024679	-0.054086	4.815588
260.656888	8000.263613	13.029683	-0.054090	4.815578
260.784516	8000.314863	13.034688	-0.054114	4.815592
260.744536	8000.288586	13.039693	-0.054106	4.815585
260.844485	8000.336177	13.044698	-0.054125	4.815598
260.966981	8000.304019	13.049703	-0.054148	4.815588
260.701361	8000.306087	13.054707	-0.054099	4.815590
260.723063	8000.298982	13.059712	-0.054103	4.815588
260.653642	8000.256198	13.064717	-0.054090	4.815576
260.738176	8000.299263	13.069722	-0.054106	4.815588
260.776188	8000.347975	13.074727	-0.054114	4.815602
260.668699	8000.268245	13.079731	-0.054094	4.815579
260.727870	8000.349352	13.084736	-0.054105	4.815603
260.612347	8000.372043	13.089741	-0.054084	4.815610
260.505509	8000.315826	13.094746	-0.054064	4.815594
260.611913	8000.367796	13.099751	-0.054084	4.815609
260.523312	8000.310810	13.104755	-0.054068	4.815592
260.369264	8000.352098	13.109760	-0.054039	4.815605
260.500012	8000.297642	13.114765	-0.054064	4.815589
260.596237	8000.308851	13.119770	-0.054082	4.815592
260.662991	8000.371922	13.124775	-0.054094	4.815610
260.568630	8000.328728	13.129779	-0.054077	4.815597
260.851119	8000.386793	13.134784	-0.054130	4.815613
260.746612	8000.300702	13.139789	-0.054111	4.815588
260.859772	8000.286551	13.144794	-0.054132	4.815584
260.956712	8000.347981	13.149799	-0.054150	4.815601
260.772896	8000.293705	13.154803	-0.054116	4.815586
260.876767	8000.306108	13.159808	-0.054136	4.815589
260.793600	8000.253484	13.164813	-0.054120	4.815574
260.910797	8000.275720	13.169818	-0.054142	4.815580
260.862813	8000.305929	13.174823	-0.054133	4.815589
260.732128	8000.258935	13.179827	-0.054109	4.815576
260.774878	8000.271404	13.184832	-0.054117	4.815580
260.727077	8000.271704	13.189837	-0.054109	4.815580
260.644553	8000.297073	13.194842	-0.054094	4.815588
260.923202	8000.262136	13.199847	-0.054146	4.815576
260.759408	8000.273353	13.204851	-0.054115	4.815580
260.830342	8000.294830	13.209856	-0.054129	4.815586
260.710417	8000.309971	13.214861	-0.054107	4.815591
260.972330	8000.318558	13.219866	-0.054156	4.815592
260.931751	8000.298680	13.224871	-0.054148	4.815587
260.669371	8000.265549	13.229875	-0.054100	4.815578
260.733011	8000.305067	13.234880	-0.054112	4.815590
260.691347	8000.243509	13.239885	-0.054104	4.815572
260.771151	8000.253381	13.244890	-0.054119	4.815574
260.861104	8000.305081	13.249895	-0.054136	4.815589
260.847003	8000.295252	13.254899	-0.054134	4.815586
260.666511	8000.339311	13.259904	-0.054100	4.815600
260.627904	8000.339763	13.264909	-0.054093	4.815600
260.581158	8000.308033	13.269914	-0.054085	4.815591
260.719987	8000.325283	13.274919	-0.054111	4.815596
260.592023	8000.264446	13.279923	-0.054087	4.815578
260.777628	8000.285667	13.284928	-0.054122	4.815584
260.618176	8000.284136	13.289933	-0.054092	4.815584
260.516136	8000.271797	13.294938	-0.054073	4.815581
260.614468	8000.287314	13.299943	-0.054092	4.815585
260.813541	8000.277777	13.304947	-0.054129	4.815581
260.812853	8000.275646	13.309952	-0.054129	4.815581
260.689814	8000.259756	13.314957	-0.054107	4.815577
260.791043	8000.293481	13.319962	-0.054126	4.815586
261.065504	8000.324708	13.324967	-0.054177	4.815594
260.862000	8000.281859	13.329971	-0.054139	4.815582
260.857988	8000.315995	13.334976	-0.054139	4.815592
260.978067	8000.285933	13.339981	-0.054161	4.815583
260.881267	8000.281157	13.344986	-0.054143	4.815582
260.936860	8000.276744	13.349991	-0.054154	4.815580
260.734457	8000.271304	13.354995	-0.054116	4.815580
260.889321	8000.295226	13.360000	-0.054145	4.815586
260.861119	8000.272347	13.365005	-0.054140	4.815579
261.001680	8000.288557	13.370010	-0.054167	4.815583
260.986344	8000.294731	13.375015	-0.054164	4.815585
260.823804	8000.254692	13.380019	-0.054134	4.815574
260.805194	8000.298202	13.385024	-0.054131	4.815587
261.115728	8000.285153	13.390029	-0.054189	4.815582
260.946104	8000.278113	13.395034	-0.054157	4.815581
260.963637	8000.294442	13.400039	-0.054161	4.815585
260.942811	8000.244976	13.405043	-0.054157	4.815571
260.998790	8000.295052	13.410048	-0.054168	4.815585
260.867496	8000.272617	13.415053	-0.054143	4.815579
260.748607	8000.246113	13.420058	-0.054121	4.815572
260.817947	8000.266496	13.425063	-0.054135	4.815578
260.583938	8000.248786	13.430067	-0.054091	4.815574
260.740806	8000.299448	13.435072	-0.054121	4.815588
260.842131	8000.275489	13.440077	-0.054140	4.815580
260.828842	8000.280628	13.445082	-0.054137	4.815582
260.962480	8000.298861	13.450087	-0.054162	4.815587
260.897674	8000.299951	13.455091	-0.054151	4.815587
260.947104	8000.320008	13.460096	-0.054160	4.815593
260.965382	8000.318188	13.465101	-0.054163	4.815592
260.953096	8000.268862	13.470106	-0.054161	4.815578
260.923789	8000.291900	13.475111	-0.054156	4.815585
260.817767	8000.249583	13.480115	-0.054137	4.815573
260.894566	8000.317092	13.485120	-0.054151	4.815592
261.068670	8000.285781	13.490125	-0.054184	4.815582
261.016662	8000.297763	13.495130	-0.054174	4.815586
260.877842	8000.307253	13.500135	-0.054149	4.815589
260.737405	8000.262235	13.505139	-0.054123	4.815577
260.905832	8000.295994	13.510144	-0.054154	4.815586
260.694764	8000.295753	13.515149	-0.054115	4.815587
260.743375	8000.302977	13.520154	-0.054124	4.815589
260.851310	8000.359246	13.525159	-0.054145	4.815605
260.742818	8000.296591	13.530163	-0.054124	4.815587
260.826712	8000.312940	13.535168	-0.054140	4.815591
261.084871	8000.271256	13.540173	-0.054189	4.815578
260.794999	8000.300702	13.545178	-0.054135	4.815588
260.837805	8000.297147	13.550183	-0.054143	4.815587
260.686122	8000.283993	13.555187	-0.054115	4.815583
260.814034	8000.283971	13.560192	-0.054139	4.815583
261.001724	8000.300955	13.565197	-0.054174	4.815587
260.823803	8000.291643	13.570202	-0.054141	4.815585
260.995418	8000.327591	13.575207	-0.054173	4.815595
260.785915	8000.307078	13.580211	-0.054134	4.815590
260.807767	8000.302112	13.585216	-0.054139	4.815588
261.058670	8000.297699	13.590221	-0.054186	4.815586
260.940369	8000.282955	13.595226	-0.054164	4.815582
260.824063	8000.334477	13.600231	-0.054142	4.815597
260.829875	8000.279039	13.605235	-0.054144	4.815581
260.896992	8000.335707	13.610240	-0.054156	4.815597
260.794855	8000.343662	13.615245	-0.054137	4.815600
260.956265	8000.323893	13.620250	-0.054168	4.815594
261.136825	8000.341828	13.625255	-0.054201	4.815598
261.037599	8000.333807	13.630259	-0.054183	4.815596
261.037802	8000.324213	13.635264	-0.054183	4.815593
261.139569	8000.278895	13.640269	-0.054202	4.815580
261.073595	8000.321628	13.645274	-0.054190	4.815592
261.154588	8000.313359	13.650279	-0.054206	4.815590
261.022107	8000.285564	13.655283	-0.054181	4.815582
261.129515	8000.320459	13.660288	-0.054201	4.815592
261.046449	8000.321249	13.665293	-0.054186	4.815592
260.980268	8000.310565	13.670298	-0.054174	4.815590
261.059491	8000.299063	13.675303	-0.054189	4.815586
260.784818	8000.290299	13.680307	-0.054138	4.815585
260.767963	8000.296449	13.685312	-0.054135	4.815587
260.586999	8000.280678	13.690317	-0.054101	4.815583
260.173026	8000.287791	13.695322	-0.054025	4.815587
260.465753	8000.302223	13.700327	-0.054079	4.815590
260.370659	8000.251540	13.705331	-0.054062	4.815575
260.774734	8000.301984	13.710336	-0.054137	4.815588
260.942263	8000.315432	13.715341	-0.054169	4.815591
260.320688	8000.272136	13.720346	-0.054053	4.815582
260.711373	8000.323428	13.725351	-0.054126	4.815595
260.749942	8000.287756	13.730355	-0.054133	4.815584
260.714360	8000.307486	13.735360	-0.054127	4.815590
260.866365	8000.302519	13.740365	-0.054155	4.815588
260.808018	8000.284486	13.745370	-0.054145	4.815583
260.875187	8000.296287	13.750375	-0.054157	4.815586
260.493739	8000.262271	13.755379	-0.054087	4.815578
260.557716	8000.302863	13.760384	-0.054099	4.815589
260.790976	8000.278931	13.765389	-0.054142	4.815581
260.857917	8000.281114	13.770394	-0.054155	4.815582
260.992554	8000.283340	13.775399	-0.054180	4.815582
260.703405	8000.271135	13.780403	-0.054127	4.815579
260.640570	8000.277598	13.785408	-0.054115	4.815582
260.870721	8000.303824	13.790413	-0.054158	4.815588
261.007252	8000.303944	13.795418	-0.054184	4.815587
260.870527	8000.320947	13.800423	-0.054158	4.815593
260.588650	8000.289632	13.805427	-0.054106	4.815585
260.770703	8000.330024	13.810432	-0.054140	4.815596
260.781313	8000.348376	13.815437	-0.054142	4.815601
260.670782	8000.307053	13.820442	-0.054122	4.815590
261.042040	8000.309956	13.825447	-0.054191	4.815589
261.098648	8000.285263	13.830451	-0.054202	4.815582
260.971627	8000.329131	13.835456	-0.054179	4.815595
260.821748	8000.317074	13.840461	-0.054151	4.815592
260.900350	8000.295947	13.845466	-0.054166	4.815586
261.071292	8000.314792	13.850471	-0.054198	4.815590
260.853380	8000.264229	13.855475	-0.054157	4.815577
260.784363	8000.315459	13.860480	-0.054145	4.815592
260.994840	8000.356318	13.865485	-0.054184	4.815603
261.028952	8000.299208	13.870490	-0.054191	4.815586
261.096824	8000.312089	13.875495	-0.054203	4.815589
261.046822	8000.304876	13.880499	-0.054194	4.815587
260.855781	8000.294280	13.885504	-0.054159	4.815585
260.690090	8000.293714	13.890509	-0.054128	4.815586
260.889934	8000.288464	13.895514	-0.054166	4.815583
261.102825	8000.320817	13.900519	-0.054205	4.815592
260.740392	8000.295658	13.905523	-0.054138	4.815586
260.848073	8000.357264	13.910528	-0.054158	4.815604
261.043344	8000.311344	13.915533	-0.054195	4.815589
260.942685	8000.301163	13.920538	-0.054176	4.815587
260.935003	8000.328828	13.925543	-0.054175	4.815595
260.801253	8000.289261	13.930547	-0.054150	4.815584
260.948360	8000.306647	13.935552	-0.054178	4.815588
260.824951	8000.321731	13.940557	-0.054155	4.815593
260.925405	8000.292416	13.945562	-0.054174	4.815584
261.098469	8000.341208	13.950567	-0.054207	4.815598
260.929350	8000.272217	13.955571	-0.054175	4.815578
261.097268	8000.316651	13.960576	-0.054207	4.815591
261.221022	8000.329381	13.965581	-0.054230	4.815594
261.126882	8000.312897	13.970586	-0.054213	4.815589
261.043180	8000.300858	13.975591	-0.054197	4.815586
260.907769	8000.286901	13.980595	-0.054172	4.815583
260.928551	8000.310761	13.985600	-0.054176	4.815590
260.878029	8000.280037	13.990605	-0.054167	4.815581
260.821077	8000.282324	13.995610	-0.054157	4.815582
260.931321	8000.285218	14.000615	-0.054177	4.815582
260.718446	8000.307380	14.005619	-0.054138	4.815590
260.832848	8000.297522	14.010624	-0.054159	4.815586
260.991766	8000.293737	14.015629	-0.054189	4.815584
260.714746	8000.281731	14.020634	-0.054138	4.815582
260.814575	8000.318638	14.025639	-0.054156	4.815592
260.844780	8000.284965	14.030643	-0.054162	4.815582
260.861999	8000.301288	14.035648	-0.054166	4.815587
260.846547	8000.288232	14.040653	-0.054163	4.815583
260.771771	8000.293432	14.045658	-0.054149	4.815585
260.896094	8000.300829	14.050663	-0.054173	4.815587
260.924128	8000.295965	14.055667	-0.054178	4.815585
260.995268	8000.318514	14.060672	-0.054191	4.815592
261.129116	8000.299361	14.065677	-0.054217	4.815585
261.028838	8000.277435	14.070682	-0.054198	4.815579
261.182483	8000.305612	14.075687	-0.054227	4.815587
261.048730	8000.282068	14.080691	-0.054202	4.815581
260.952255	8000.289048	14.085696	-0.054184	4.815583
260.853658	8000.303470	14.090701	-0.054166	4.815588
260.797032	8000.280124	14.095706	-0.054156	4.815581
260.909136	8000.342872	14.100711	-0.054177	4.815599
260.702585	8000.332021	14.105715	-0.054139	4.815597
260.801838	8000.324052	14.110720	-0.054157	4.815594
260.989202	8000.329279	14.115725	-0.054192	4.815595
260.833892	8000.304314	14.120730	-0.054164	4.815588
260.867593	8000.334795	14.125735	-0.054170	4.815597
260.864319	8000.315529	14.130739	-0.054170	4.815591
260.935833	8000.298558	14.135744	-0.054183	4.815586
260.814804	8000.314750	14.140749	-0.054161	4.815591
260.721180	8000.300411	14.145754	-0.054144	4.815587
260.952192	8000.327720	14.150759	-0.054187	4.815594
261.060550	8000.300671	14.155763	-0.054207	4.815586
261.063020	8000.324230	14.160768	-0.054208	4.815593
261.079820	8000.325591	14.165773	-0.054211	4.815593
260.960636	8000.316174	14.170778	-0.054189	4.815591
260.916068	8000.343234	14.175783	-0.054181	4.815599
260.746852	8000.316972	14.180787	-0.054150	4.815592
260.815507	8000.330934	14.185792	-0.054163	4.815596
260.884570	8000.355586	14.190797	-0.054176	4.815603
260.995887	8000.306152	14.195802	-0.054197	4.815588
261.114739	8000.342304	14.200807	-0.054219	4.815598
260.868168	8000.366049	14.205811	-0.054173	4.815606
261.014474	7999.317317	14.210816	-0.054200	4.815299
260.987939	7996.123269	14.215821	-0.054193	4.814365
260.784403	7990.565200	14.220826	-0.054152	4.812741
260.840113	7983.925707	14.225831	-0.054158	4.810799
260.930788	7976.630186	14.230835	-0.054170	4.808664
260.936941	7969.007087	14.235840	-0.054167	4.806432
260.961612	7961.213040	14.240845	-0.054166	4.804149
260.805514	7953.321937	14.245850	-0.054132	4.801838
260.714522	7945.369671	14.250855	-0.054111	4.799507
260.582677	7937.465397	14.255859	-0.054081	4.797189
260.496248	7929.377404	14.260864	-0.054060	4.794816
260.678117	7921.431298	14.265869	-0.054089	4.792482
260.699809	7913.328384	14.270874	-0.054088	4.790102
260.630954	7905.421516	14.275879	-0.054070	4.787779
260.541183	7897.374920	14.280883	-0.054048	4.785413
260.619063	7889.431200	14.285888	-0.054058	4.783076
260.508615	7881.431525	14.290893	-0.054032	4.780722
260.423642	7873.384241	14.295898	-0.054011	4.778353
260.602735	7865.430276	14.300903	-0.054039	4.776009
260.447814	7857.390057	14.305907	-0.054006	4.773640
260.409362	7849.367025	14.310912	-0.053993	4.771274
260.305734	7841.365161	14.315917	-0.053969	4.768913
260.335786	7833.336182	14.320922	-0.053970	4.766543
260.421360	7825.357313	14.325927	-0.053981	4.764186
260.238726	7817.420350	14.330931	-0.053942	4.761842
260.146142	7809.369133	14.335936	-0.053919	4.759462
260.127062	7801.417811	14.340941	-0.053911	4.757110
259.956441	7793.342143	14.345946	-0.053874	4.754721
260.080283	7785.305532	14.350951	-0.053892	4.752341
260.087119	7777.300069	14.355955	-0.053888	4.749969
259.897702	7769.310177	14.360960	-0.053848	4.747602
259.681602	7761.338804	14.365965	-0.053803	4.745239
259.735624	7753.370101	14.370970	-0.053808	4.742874
259.998545	7745.350715	14.375975	-0.053852	4.740493
259.879391	7737.346143	14.380979	-0.053824	4.738117
259.840117	7729.296005	14.385984	-0.053812	4.735725
259.712072	7721.361444	14.390989	-0.053783	4.733366
259.663254	7713.336147	14.395994	-0.053769	4.730980
259.671712	7705.323849	14.400999	-0.053766	4.728595
259.506252	7697.285714	14.406003	-0.053730	4.726203
259.387450	7689.315005	14.411008	-0.053703	4.723829
259.488222	7681.305229	14.416013	-0.053716	4.721441
259.631324	7673.312395	14.421018	-0.053738	4.719058
259.485965	7665.361962	14.426023	-0.053706	4.716686
259.277224	7657.271817	14.431027	-0.053662	4.714272
259.289424	7649.305756	14.436032	-0.053659	4.711893
259.287205	7641.304959	14.441037	-0.053654	4.709502
259.312062	7633.270849	14.446042	-0.053653	4.707101
259.237039	7625.299589	14.451047	-0.053634	4.704717
259.356397	7617.331708	14.456051	-0.053652	4.702332
259.278292	7609.275762	14.461056	-0.053632	4.699920
259.271356	7601.365136	14.466061	-0.053626	4.697551
259.296270	7593.254598	14.471066	-0.053625	4.695120
259.098908	7585.304021	14.476071	-0.053583	4.692736
258.954491	7577.264262	14.481075	-0.053552	4.690325
258.964952	7569.278498	14.486080	-0.053548	4.687927
259.187274	7561.279340	14.491085	-0.053585	4.685525
258.879783	7553.288520	14.496090	-0.053523	4.683124
258.966403	7545.340386	14.501095	-0.053534	4.680735
258.922868	7537.294953	14.506099	-0.053521	4.678315
258.821379	7529.273123	14.511104	-0.053497	4.675901
258.738018	7521.236912	14.516109	-0.053476	4.673481
258.628904	7513.140548	14.521114	-0.053451	4.671042
258.901729	7505.210659	14.526119	-0.053496	4.668652
258.754941	7497.227069	14.531123	-0.053464	4.666245
258.678245	7489.232431	14.536128	-0.053445	4.663833
258.887298	7481.236860	14.541133	-0.053479	4.661419
258.790321	7473.213240	14.546138	-0.053456	4.658995
258.740893	7465.242549	14.551143	-0.053441	4.656587
258.667951	7457.223284	14.556147	-0.053423	4.654162
258.556505	7449.201926	14.561152	-0.053397	4.651736
258.469239	7441.173530	14.566157	-0.053376	4.649306
258.345499	7433.221423	14.571162	-0.053348	4.646898
258.505889	7425.214452	14.576167	-0.053373	4.644472
258.476681	7417.275012	14.581171	-0.053362	4.642065
258.411818	7409.200709	14.586176	-0.053345	4.639616
258.417080	7401.270716	14.591181	-0.053341	4.637210
258.241174	7393.178000	14.596186	-0.053303	4.634753
258.182469	7385.178190	14.601191	-0.053287	4.632322
258.236608	7377.168382	14.606195	-0.053292	4.629888
258.206322	7369.185258	14.611200	-0.053282	4.627460
258.076015	7361.208302	14.616205	-0.053252	4.625033
258.188528	7353.205013	14.621210	-0.053268	4.622597
258.095410	7345.179152	14.626215	-0.053246	4.620152
257.954707	7337.193412	14.631219	-0.053215	4.617719
257.900949	7329.142352	14.636224	-0.053200	4.615264
258.023004	7321.189723	14.641229	-0.053217	4.612838
257.804592	7313.138037	14.646234	-0.053172	4.610380
257.858649	7305.136614	14.651239	-0.053177	4.607936
257.932723	7297.142474	14.656243	-0.053185	4.605494
257.912299	7289.193468	14.661248	-0.053177	4.603064
257.848827	7281.178312	14.666253	-0.053160	4.600612
257.704263	7273.210392	14.671258	-0.053128	4.598173
257.888414	7265.203496	14.676263	-0.053157	4.595722
257.690361	7257.120932	14.681267	-0.053115	4.593245
257.599198	7249.068079	14.686272	-0.053093	4.590777
257.588938	7241.156822	14.691277	-0.053086	4.588350
257.292966	7233.093747	14.696282	-0.053026	4.585876
257.367020	7225.172526	14.701287	-0.053035	4.583444
257.455445	7217.142674	14.706291	-0.053046	4.580977
257.357531	7209.139972	14.711296	-0.053023	4.578517
257.333821	7201.134295	14.716301	-0.053013	4.576055
257.419439	7193.105213	14.721306	-0.053024	4.573585
257.555005	7185.087375	14.726311	-0.053045	4.571117
257.437655	7177.143615	14.731315	-0.053018	4.568669
257.194248	7169.107412	14.736320	-0.052967	4.566192
257.207502	7161.117180	14.741325	-0.052965	4.563729
257.147887	7153.137634	14.746330	-0.052949	4.561267
256.934190	7145.145902	14.751335	-0.052904	4.558799
256.924561	7137.188997	14.756339	-0.052897	4.556342
257.166222	7129.105945	14.761344	-0.052937	4.553844
257.116875	7121.082158	14.766349	-0.052923	4.551363
257.013994	7113.091294	14.771354	-0.052899	4.548891
256.934278	7105.113775	14.776359	-0.052879	4.546421
256.889729	7097.073926	14.781363	-0.052865	4.543931
256.735002	7089.112657	14.786368	-0.052832	4.541464
256.878498	7081.141961	14.791373	-0.052853	4.538993
256.876890	7073.124115	14.796378	-0.052848	4.536505
256.926765	7065.090244	14.801383	-0.052852	4.534012
256.676976	7057.080796	14.806387	-0.052801	4.531524
256.633719	7049.068459	14.811392	-0.052788	4.529034
256.710003	7041.154104	14.816397	-0.052797	4.526574
256.570667	7033.092029	14.821402	-0.052766	4.524065
256.707276	7025.187933	14.826407	-0.052786	4.521606
256.417292	7017.127882	14.831411	-0.052727	4.519095
256.266465	7009.145499	14.836416	-0.052694	4.516607
256.288383	7001.075136	14.841421	-0.052693	4.514091
256.399956	6993.018563	14.846426	-0.052709	4.511578
256.244804	6985.021621	14.851431	-0.052675	4.509082
256.091304	6977.054148	14.856435	-0.052641	4.506593
256.336889	6969.017808	14.861440	-0.052682	4.504083
256.239973	6961.111651	14.866445	-0.052659	4.501611
256.106868	6953.013644	14.871450	-0.052629	4.499078
256.377912	6945.091079	14.876455	-0.052675	4.496599
256.284090	6937.064561	14.881459	-0.052652	4.494085
256.159249	6929.067778	14.886464	-0.052624	4.491579
256.254780	6921.028574	14.891469	-0.052637	4.489059
256.128896	6913.037838	14.896474	-0.052608	4.486552
256.206860	6905.047577	14.901479	-0.052618	4.484044
256.008847	6897.073549	14.906483	-0.052576	4.481539
255.865033	6889.055818	14.911488	-0.052544	4.479020
256.015433	6881.081215	14.916493	-0.052567	4.476513
255.804040	6873.037573	14.921498	-0.052523	4.473982
255.816164	6865.025847	14.926503	-0.052520	4.471460
255.652726	6857.023595	14.931507	-0.052484	4.468940
255.585369	6849.017895	14.936512	-0.052467	4.466417
255.609628	6841.072112	14.941517	-0.052466	4.463912
255.587604	6833.026462	14.946522	-0.052457	4.461373
255.725004	6825.030950	14.951527	-0.052478	4.458850
255.667805	6817.042299	14.956531	-0.052462	4.456327
255.655536	6809.016161	14.961536	-0.052455	4.453791
255.666922	6800.983451	14.966541	-0.052452	4.451251
255.343167	6793.013885	14.971546	-0.052386	4.448728
255.376697	6784.994041	14.976551	-0.052388	4.446190
255.339683	6777.031930	14.981555	-0.052376	4.443668
255.212818	6769.014504	14.986560	-0.052347	4.441127
255.519689	6761.065716	14.991565	-0.052399	4.438607
255.133774	6753.003974	14.996570	-0.052322	4.436048
255.018054	6745.006191	15.001575	-0.052296	4.433509
254.956109	6736.951361	15.006579	-0.052279	4.430950
255.109471	6728.946241	15.011584	-0.052303	4.428406
255.318043	6720.923272	15.016589	-0.052336	4.425856
255.132902	6712.998943	15.021594	-0.052297	4.423334
255.256067	6705.013826	15.026599	-0.052315	4.420792
255.183285	6697.008792	15.031603	-0.052296	4.418242
254.826256	6688.987316	15.036608	-0.052225	4.415683
254.755396	6680.994576	15.041613	-0.052207	4.413134
254.725496	6672.960855	15.046618	-0.052196	4.410570
254.757170	6664.969945	15.051623	-0.052197	4.408019
254.771520	6656.958535	15.056627	-0.052195	4.405459
254.817554	6648.981533	15.061632	-0.052198	4.402910
254.846185	6640.991865	15.066637	-0.052198	4.400354
254.661989	6632.999658	15.071642	-0.052159	4.397795
254.586690	6625.002548	15.076647	-0.052140	4.395234
254.696122	6616.996268	15.081651	-0.052155	4.392669
254.579640	6608.961536	15.086656	-0.052129	4.390093
254.592919	6600.986713	15.091661	-0.052126	4.387535
254.384952	6592.922241	15.096666	-0.052082	4.384945
254.364649	6585.006013	15.101671	-0.052074	4.382402
254.304895	6576.968848	15.106675	-0.052057	4.379819
254.351563	6568.983048	15.111680	-0.052061	4.377252
254.453756	6560.994108	15.116685	-0.052075	4.374682
254.398298	6552.972046	15.121690	-0.052060	4.372099
254.449188	6544.940157	15.126695	-0.052064	4.369512
254.607685	6537.009739	15.131699	-0.052089	4.366957
254.342887	6528.962353	15.136704	-0.052034	4.364360
254.485170	6521.068660	15.141709	-0.052056	4.361814
254.455192	6513.005041	15.146714	-0.052045	4.359210
254.390791	6504.993310	15.151719	-0.052028	4.356621
254.477142	6496.949572	15.156723	-0.052039	4.354022
254.324869	6488.848846	15.161728	-0.052006	4.351401
254.352159	6480.890204	15.166733	-0.052006	4.348825
254.056078	6472.925575	15.171738	-0.051946	4.346244
254.145854	6464.958758	15.176743	-0.051957	4.343663
254.204875	6456.991517	15.181747	-0.051963	4.341080
254.115933	6448.955167	15.186752	-0.051942	4.338472
253.981820	6440.980420	15.191757	-0.051912	4.335882
253.890304	6432.946165	15.196762	-0.051890	4.333272
253.835513	6424.913116	15.201767	-0.051874	4.330661
253.805786	6416.957330	15.206771	-0.051864	4.328073
253.712050	6408.913742	15.211776	-0.051841	4.325455
253.799896	6400.966874	15.216781	-0.051853	4.322868
253.743163	6392.927400	15.221786	-0.051837	4.320249
253.786515	6384.968111	15.226791	-0.051840	4.317654
253.735469	6376.943038	15.231795	-0.051826	4.315036
253.685858	6368.912313	15.236800	-0.051811	4.312415
253.498589	6360.937484	15.241805	-0.051772	4.309809
253.534468	6352.905021	15.246810	-0.051773	4.307184
253.447622	6344.921394	15.251815	-0.051752	4.304573
253.577599	6336.995669	15.256819	-0.051771	4.301981
253.356714	6328.909610	15.261824	-0.051725	4.299331
253.404773	6320.967879	15.266829	-0.051729	4.296730
253.344157	6312.929816	15.271834	-0.051713	4.294095
253.353464	6304.892143	15.276839	-0.051709	4.291459
253.191710	6296.917865	15.281843	-0.051674	4.288840
253.180737	6288.865874	15.286848	-0.051667	4.286196
253.037997	6280.953259	15.291853	-0.051636	4.283595
252.962738	6272.914707	15.296858	-0.051616	4.280951
253.168661	6264.945108	15.301863	-0.051650	4.278331
253.115428	6256.946234	15.306867	-0.051635	4.275697
253.203082	6248.852015	15.311872	-0.051646	4.273031
253.119617	6240.890392	15.316877	-0.051626	4.270406
253.029963	6232.870467	15.321882	-0.051604	4.267761
252.792919	6224.850019	15.326887	-0.051555	4.265112
252.828139	6216.923771	15.331891	-0.051556	4.262494
252.756734	6208.899472	15.336896	-0.051538	4.259842
252.906062	6200.946897	15.341901	-0.051561	4.257214
252.737090	6192.901284	15.346906	-0.051524	4.254551
252.540747	6184.876623	15.351911	-0.051483	4.251892
252.584349	6176.890926	15.356915	-0.051486	4.249247
252.485444	6168.894398	15.361920	-0.051462	4.246596
252.598348	6160.913895	15.366925	-0.051478	4.243950
252.645351	6152.914805	15.371930	-0.051482	4.241296
252.683699	6144.940693	15.376935	-0.051484	4.238648
252.470753	6136.951529	15.381939	-0.051439	4.235991
252.518479	6128.895176	15.386944	-0.051443	4.233313
252.457617	6120.882713	15.391949	-0.051427	4.230646
252.474184	6112.919000	15.396954	-0.051425	4.227995
252.544456	6104.888438	15.401959	-0.051433	4.225320
252.454998	6096.969728	15.406963	-0.051411	4.222680
252.446690	6088.897338	15.411968	-0.051405	4.219987
252.469629	6080.969430	15.416973	-0.051404	4.217341
252.369673	6072.913779	15.421978	-0.051380	4.214650
252.335468	6064.942568	15.426983	-0.051369	4.211985
252.089277	6056.900787	15.431987	-0.051318	4.209294
252.178010	6048.932278	15.436992	-0.051330	4.206628
252.141770	6040.966143	15.441997	-0.051318	4.203960
252.065334	6032.934616	15.447002	-0.051299	4.201268
251.982256	6024.974577	15.452007	-0.051278	4.198599
252.165256	6016.960069	15.457011	-0.051307	4.195912
252.051043	6008.808534	15.462016	-0.051281	4.193174
252.218865	6000.803869	15.467021	-0.051307	4.190487
252.038411	5992.880479	15.472026	-0.051268	4.187822
251.795927	5984.894628	15.477031	-0.051218	4.185133
251.582978	5976.921400	15.482035	-0.051174	4.182447
251.515524	5968.891166	15.487040	-0.051156	4.179742
251.723299	5960.938592	15.492045	-0.051190	4.177064
251.629735	5952.898297	15.497050	-0.051167	4.174352
251.665644	5944.902428	15.502055	-0.051169	4.171654
251.700102	5936.879422	15.507059	-0.051170	4.168946
251.489947	5928.901279	15.512064	-0.051126	4.166248
251.525181	5920.903457	15.517069	-0.051128	4.163544
251.512212	5912.882948	15.522074	-0.051120	4.160830
251.443791	5904.919369	15.527079	-0.051102	4.158134
251.378692	5896.942450	15.532083	-0.051085	4.155431
251.213736	5888.857294	15.537088	-0.051050	4.152688
251.354494	5880.868095	15.542093	-0.051071	4.149980
251.222436	5872.889955	15.547098	-0.051041	4.147270
251.139451	5864.865740	15.552103	-0.051021	4.144544
251.188467	5856.927563	15.557107	-0.051025	4.141846
251.079720	5848.883627	15.562112	-0.051000	4.139109
251.167490	5840.936143	15.567117	-0.051011	4.136405
251.142261	5832.877843	15.572122	-0.051001	4.133661
251.002517	5824.857455	15.577127	-0.050970	4.130926
251.048296	5816.886021	15.582131	-0.050974	4.128208
250.876459	5808.850967	15.587136	-0.050937	4.125464
251.006373	5800.920821	15.592141	-0.050956	4.122758
250.787226	5792.884532	15.597146	-0.050910	4.120010
250.743026	5784.939387	15.602151	-0.050897	4.117292
250.849666	5776.937313	15.607155	-0.050911	4.114556
250.654465	5768.833369	15.612160	-0.050870	4.111779
250.777587	5760.867800	15.617165	-0.050888	4.109052
250.806143	5752.854626	15.622170	-0.050888	4.106305
250.700453	5744.880138	15.627175	-0.050864	4.103568
250.622749	5736.881762	15.632179	-0.050844	4.100821
250.591726	5728.906972	15.637184	-0.050833	4.098081
250.657969	5720.904712	15.642189	-0.050841	4.095331
250.509411	5712.925246	15.647194	-0.050808	4.092585
250.501813	5704.889473	15.652199	-0.050801	4.089819
250.610803	5696.927046	15.657203	-0.050817	4.087077
250.464809	5688.858670	15.662208	-0.050784	4.084294
250.352499	5680.942014	15.667213	-0.050759	4.081562
250.094870	5672.927099	15.672218	-0.050706	4.078793
250.182989	5664.947246	15.677223	-0.050717	4.076038
250.191097	5656.952506	15.682227	-0.050713	4.073275
250.103285	5648.870523	15.687232	-0.050692	4.070478
250.134291	5640.928175	15.692237	-0.050693	4.067730
250.222151	5632.902352	15.697242	-0.050704	4.064952
249.916602	5624.955784	15.702247	-0.050642	4.062194
250.046532	5616.923877	15.707251	-0.050661	4.059410
249.732454	5608.959013	15.712256	-0.050598	4.056641
249.815517	5600.971494	15.717261	-0.050608	4.053869
249.953397	5592.928742	15.722266	-0.050629	4.051076
249.719680	5584.923267	15.727271	-0.050580	4.048288
249.885153	5576.923586	15.732275	-0.050606	4.045507
249.752419	5568.936623	15.737280	-0.050577	4.042724
249.930971	5560.927622	15.742285	-0.050605	4.039936
249.636805	5552.977440	15.747290	-0.050545	4.037159
249.515373	5544.919893	15.752295	-0.050517	4.034345
249.495438	5536.838614	15.757299	-0.050508	4.031523
249.385998	5528.842808	15.762304	-0.050483	4.028727
249.445354	5520.862203	15.767309	-0.050489	4.025937
249.365473	5512.924424	15.772314	-0.050469	4.023158
249.520622	5504.917663	15.777319	-0.050493	4.020357
249.273934	5496.943083	15.782323	-0.050442	4.017559
249.478554	5488.889173	15.787328	-0.050475	4.014738
249.407887	5480.901140	15.792333	-0.050457	4.011934
249.359921	5472.879496	15.797338	-0.050443	4.009116
249.379035	5464.891587	15.802343	-0.050442	4.006309
249.391273	5456.937097	15.807347	-0.050439	4.003512
249.203355	5448.900574	15.812352	-0.050399	4.000681
249.079695	5440.970589	15.817357	-0.050371	3.997887
249.012723	5432.922286	15.822362	-0.050353	3.995050
249.086356	5424.882128	15.827367	-0.050362	3.992215
249.050877	5416.885408	15.832371	-0.050350	3.989393
248.743231	5408.916694	15.837376	-0.050288	3.986574
248.954491	5400.911960	15.842381	-0.050322	3.983748
248.860189	5392.932387	15.847386	-0.050300	3.980925
248.854970	5384.935825	15.852391	-0.050294	3.978095
248.911347	5376.952638	15.857395	-0.050299	3.975268
248.838688	5368.897555	15.862400	-0.050281	3.972412
248.738251	5360.927058	15.867405	-0.050257	3.969584
248.681170	5352.949671	15.872410	-0.050241	3.966751
248.552031	5344.953343	15.877415	-0.050212	3.963909
248.405142	5336.990885	15.882419	-0.050180	3.961077
248.460234	5328.956007	15.887424	-0.050185	3.958220
248.723514	5320.961546	15.892429	-0.050229	3.955379
248.509855	5312.936339	15.897434	-0.050184	3.952516
248.285725	5304.893914	15.902439	-0.050138	3.949646
248.107362	5296.979428	15.907443	-0.050099	3.946819
248.151012	5288.957480	15.912448	-0.050102	3.943956
248.127293	5281.006700	15.917453	-0.050093	3.941116
248.244548	5272.988330	15.922458	-0.050110	3.938251
248.225883	5264.963327	15.927463	-0.050101	3.935380
247.998834	5256.976403	15.932467	-0.050054	3.932516
247.875952	5248.929199	15.937472	-0.050026	3.929631
248.012746	5241.001966	15.942477	-0.050047	3.926791
248.089728	5232.970366	15.947482	-0.050056	3.923911
247.894621	5224.981916	15.952487	-0.050015	3.921039
247.905177	5217.028880	15.957491	-0.050011	3.918181
247.820665	5209.014477	15.962496	-0.049991	3.915298
247.802911	5201.006062	15.967501	-0.049982	3.912416
247.812500	5192.947557	15.972506	-0.049979	3.909514
247.908077	5184.970259	15.977511	-0.049992	3.906641
247.775983	5176.987251	15.982515	-0.049962	3.903759
247.458186	5168.992210	15.987520	-0.049898	3.900867
247.792012	5161.021859	15.992525	-0.049955	3.897995
247.623451	5153.008509	15.997530	-0.049919	3.895095
247.477683	5144.987924	16.002535	-0.049887	3.892191
247.603339	5136.971972	16.007539	-0.049905	3.889292
247.546928	5128.982812	16.012544	-0.049889	3.886396
247.416477	5121.009607	16.017549	-0.049860	3.883503
247.256980	5112.996650	16.022554	-0.049825	3.880593
247.528064	5105.032855	16.027559	-0.049871	3.877707
247.468194	5097.021418	16.032563	-0.049855	3.874794
247.206896	5088.752294	16.037568	-0.049801	3.871782
247.349836	5080.843403	16.042573	-0.049823	3.868907
247.107656	5072.905601	16.047578	-0.049772	3.866011
246.964408	5064.935914	16.052583	-0.049741	3.863104
247.136993	5056.954979	16.057587	-0.049768	3.860196
247.085004	5048.997474	16.062592	-0.049753	3.857291
247.144714	5040.968063	16.067597	-0.049759	3.854359
246.752295	5032.960402	16.072602	-0.049681	3.851423
246.892451	5024.963532	16.077607	-0.049702	3.848501
246.902432	5016.987616	16.082611	-0.049699	3.845581
246.735233	5009.042159	16.087616	-0.049663	3.842666
246.724387	5001.036152	16.092621	-0.049656	3.839730
246.672855	4993.075141	16.097626	-0.049641	3.836807
246.730226	4985.040134	16.102631	-0.049647	3.833858
246.679344	4977.020832	16.107635	-0.049632	3.830909
246.760443	4969.018034	16.112640	-0.049643	3.827967
246.752403	4961.018823	16.117645	-0.049636	3.825023
246.710767	4953.059899	16.122650	-0.049623	3.822090
246.770436	4945.049644	16.127655	-0.049629	3.819138
246.684909	4937.100465	16.132659	-0.049608	3.816203
246.103203	4929.094055	16.137664	-0.049495	3.813235
246.287132	4921.038667	16.142669	-0.049524	3.810262
246.355886	4913.082282	16.147674	-0.049532	3.807321
246.248884	4905.056295	16.152679	-0.049507	3.804348
246.309844	4897.141363	16.157683	-0.049513	3.801418
246.154174	4889.082783	16.162688	-0.049479	3.798427
246.321283	4881.094836	16.167693	-0.049506	3.795468
246.050683	4873.058303	16.172698	-0.049450	3.792478
246.124172	4865.059002	16.177703	-0.049459	3.789507
246.216294	4857.073230	16.182707	-0.049471	3.786540
246.002109	4849.093568	16.187712	-0.049426	3.783566
245.879856	4841.068673	16.192717	-0.049398	3.780574
246.090880	4833.101281	16.197722	-0.049432	3.777609
245.905757	4825.074482	16.202727	-0.049393	3.774611
245.895137	4817.108771	16.207731	-0.049386	3.771637
245.658016	4809.050367	16.212736	-0.049337	3.768621
245.851009	4801.099976	16.217741	-0.049368	3.765652
245.891499	4793.112571	16.222746	-0.049370	3.762664
245.844414	4785.056049	16.227751	-0.049356	3.759646
245.803412	4777.177999	16.232755	-0.049344	3.756692
245.736469	4769.106438	16.237760	-0.049326	3.753663
245.683034	4761.075505	16.242765	-0.049311	3.750647
245.768885	4753.084762	16.247770	-0.049322	3.747646
245.604695	4745.057886	16.252775	-0.049287	3.744624
245.304109	4737.168002	16.257779	-0.049226	3.741648
245.255313	4729.113784	16.262784	-0.049212	3.738614
245.409729	4721.122058	16.267789	-0.049235	3.735605
245.329211	4713.126725	16.272794	-0.049215	3.732587
245.432834	4705.080775	16.277799	-0.049230	3.729552
245.464843	4697.166469	16.282803	-0.049231	3.726562
245.078490	4689.154774	16.287808	-0.049154	3.723523
245.217996	4681.186274	16.292813	-0.049175	3.720511
245.461906	4673.194411	16.297818	-0.049215	3.717489
245.199438	4665.184700	16.302823	-0.049161	3.714447
244.926507	4657.118189	16.307827	-0.049105	3.711380
244.850233	4649.085201	16.312832	-0.049086	3.708328
244.937306	4641.119711	16.317837	-0.049097	3.705303
244.676701	4633.176755	16.322842	-0.049044	3.702275
244.631386	4625.146019	16.327847	-0.049030	3.699217
244.615356	4617.221609	16.332851	-0.049022	3.696198
244.508946	4609.190939	16.337856	-0.048997	3.693133
244.792462	4601.163392	16.342861	-0.049045	3.690077
244.756048	4593.201911	16.347866	-0.049033	3.687036
244.505677	4585.201590	16.352871	-0.048982	3.683972
244.602150	4577.252711	16.357875	-0.048995	3.680933
244.567755	4569.238383	16.362880	-0.048983	3.677864
244.642304	4561.235702	16.367885	-0.048992	3.674799
244.438548	4553.233092	16.372890	-0.048949	3.671725
244.419272	4545.233014	16.377895	-0.048940	3.668654
244.573522	4537.228767	16.382899	-0.048964	3.665583
244.324657	4529.239742	16.387904	-0.048913	3.662505
244.307925	4521.253979	16.392909	-0.048905	3.659432
244.282810	4513.282800	16.397914	-0.048895	3.656362
244.230127	4505.246536	16.402919	-0.048880	3.653263
244.106851	4497.259158	16.407923	-0.048852	3.650178
244.071616	4489.260432	16.412928	-0.048841	3.647089
244.021591	4481.265483	16.417933	-0.048826	3.643998
243.984954	4473.278036	16.422938	-0.048814	3.640908
243.954887	4465.299357	16.427943	-0.048804	3.637819
243.966416	4457.293175	16.432947	-0.048801	3.634717
243.899222	4449.226061	16.437952	-0.048783	3.631588
243.787853	4441.257471	16.442957	-0.048758	3.628492
243.793953	4433.252976	16.447962	-0.048754	3.625383
243.582541	4425.281836	16.452967	-0.048709	3.622279
243.591864	4417.306926	16.457971	-0.048706	3.619176
243.686706	4409.299971	16.462976	-0.048719	3.616061
243.890673	4401.275352	16.467981	-0.048752	3.612939
243.713363	4393.269408	16.472986	-0.048713	3.609811
243.381617	4385.315033	16.477991	-0.048647	3.606696
243.653212	4377.339861	16.482995	-0.048692	3.603587
243.591182	4369.339442	16.488000	-0.048676	3.600456
243.371768	4361.409108	16.493005	-0.048630	3.597346
243.352711	4353.376559	16.498010	-0.048621	3.594198
243.264534	4345.353653	16.503015	-0.048600	3.591050
243.157195	4337.394073	16.508019	-0.048575	3.587923
243.002881	4329.359887	16.513024	-0.048541	3.584762
243.186710	4321.385296	16.518029	-0.048570	3.581632
243.126005	4313.387822	16.523034	-0.048554	3.578483
243.019720	4305.388862	16.528039	-0.048529	3.575330
243.133722	4297.409388	16.533043	-0.048545	3.572187
243.079526	4289.385959	16.538048	-0.048530	3.569020
242.960052	4281.420317	16.543053	-0.048503	3.565871
242.755333	4273.445954	16.548058	-0.048460	3.562713
242.783116	4265.391358	16.553063	-0.048460	3.559527
242.904304	4257.484412	16.558067	-0.048478	3.556400
242.649332	4249.398956	16.563072	-0.048425	3.553188
242.737312	4241.331552	16.568077	-0.048436	3.549991
242.817755	4233.359189	16.573082	-0.048446	3.546828
242.515919	4225.377006	16.578087	-0.048385	3.543647
242.674701	4217.417739	16.583091	-0.048410	3.540486
242.730079	4209.443515	16.588096	-0.048415	3.537313
242.653633	4201.444873	16.593101	-0.048396	3.534123
242.608225	4193.418278	16.598106	-0.048382	3.530921
242.638688	4185.421376	16.603111	-0.048383	3.527729
242.629790	4177.435477	16.608115	-0.048376	3.524538
242.317552	4169.513514	16.613120	-0.048313	3.521361
242.336032	4161.482341	16.618125	-0.048311	3.518147
242.535285	4153.479693	16.623130	-0.048344	3.514947
242.472296	4145.453823	16.628135	-0.048327	3.511726
242.286062	4137.512485	16.633139	-0.048287	3.508533
242.244733	4129.488044	16.638144	-0.048274	3.505308
242.101474	4121.544093	16.643149	-0.048243	3.502109
241.959862	4113.548417	16.648154	-0.048211	3.498887
241.968972	4105.544573	16.653159	-0.048208	3.495663
242.065130	4097.535904	16.658163	-0.048221	3.492436
241.765222	4089.526919	16.663168	-0.048160	3.489195
241.914547	4081.567538	16.668173	-0.048183	3.485984
241.825029	4073.590984	16.673178	-0.048161	3.482756
241.630239	4065.601640	16.678183	-0.048120	3.479516
241.760124	4057.635008	16.683187	-0.048139	3.476293
241.699061	4049.575394	16.688192	-0.048123	3.473023
241.625035	4041.559031	16.693197	-0.048104	3.469767
241.570991	4033.597033	16.698202	-0.048089	3.466531
241.563241	4025.597367	16.703207	-0.048082	3.463278
241.784734	4017.602996	16.708211	-0.048118	3.460031
241.685822	4009.623328	16.713216	-0.048095	3.456777
241.542509	4001.627244	16.718221	-0.048063	3.453512
241.457077	3993.621134	16.723226	-0.048042	3.450241
241.240645	3985.632473	16.728231	-0.047997	3.446970
241.352329	3977.663862	16.733235	-0.048013	3.443715
241.305443	3969.655375	16.738240	-0.047999	3.440435
241.186405	3961.684791	16.743245	-0.047972	3.437166
240.999864	3953.711373	16.748250	-0.047932	3.433889
241.122446	3945.630703	16.753255	-0.047950	3.430576
241.238071	3937.681382	16.758259	-0.047966	3.427314
240.994968	3929.670397	16.763264	-0.047916	3.424011
240.929247	3921.698901	16.768269	-0.047899	3.420727
240.868599	3913.722560	16.773274	-0.047883	3.417438
241.107040	3905.691382	16.778279	-0.047922	3.414133
241.165692	3897.694862	16.783283	-0.047928	3.410834
241.101985	3889.701873	16.788288	-0.047911	3.407528
241.060273	3881.726913	16.793293	-0.047898	3.404227
240.772809	3873.808098	16.798298	-0.047840	3.400938
240.711429	3865.808913	16.803303	-0.047823	3.397621
240.844523	3857.786231	16.808307	-0.047843	3.394297
240.794591	3849.689803	16.813312	-0.047829	3.390932
240.730474	3841.739243	16.818317	-0.047812	3.387625
240.740450	3833.742235	16.823322	-0.047808	3.384297
240.513122	3825.790399	16.828327	-0.047761	3.380977
240.466897	3817.832624	16.833331	-0.047748	3.377658
240.296964	3809.814708	16.838336	-0.047711	3.374305
240.251026	3801.797271	16.843341	-0.047697	3.370954
240.222625	3793.829612	16.848346	-0.047687	3.367621
240.010814	3785.822938	16.853351	-0.047643	3.364262
240.445562	3777.865723	16.858355	-0.047718	3.360943
239.980835	3769.918341	16.863360	-0.047627	3.357593
240.030637	3761.882768	16.868365	-0.047631	3.354221
240.137375	3753.830293	16.873370	-0.047646	3.350840
240.072844	3745.855604	16.878375	-0.047629	3.347483
240.062359	3737.888708	16.883379	-0.047622	3.344127
240.051459	3729.883221	16.888384	-0.047615	3.340752
239.892545	3721.920911	16.893389	-0.047580	3.337386
239.722856	3713.930718	16.898394	-0.047544	3.334005
239.747967	3705.898463	16.903399	-0.047543	3.330609
239.807713	3697.956132	16.908403	-0.047549	3.327250
239.667772	3689.947291	16.913408	-0.047518	3.323851
239.682856	3681.958071	16.918413	-0.047516	3.320463
239.714083	3674.004975	16.923418	-0.047517	3.317088
239.754670	3665.960019	16.928423	-0.047520	3.313670
239.644613	3657.953572	16.933427	-0.047494	3.310259
239.446377	3649.975723	16.938432	-0.047452	3.306854
239.447067	3641.997260	16.943437	-0.047447	3.303453
239.458549	3634.026785	16.948442	-0.047444	3.300052
239.350617	3626.064249	16.953447	-0.047419	3.296646
239.495073	3618.036301	16.958451	-0.047441	3.293218
239.093676	3610.048908	16.963456	-0.047361	3.289783
239.223295	3602.053566	16.968461	-0.047380	3.286362
239.269302	3594.084216	16.973466	-0.047384	3.282945
239.296111	3586.076199	16.978471	-0.047384	3.279507
239.200011	3578.146496	16.983475	-0.047361	3.276094
239.188182	3570.092017	16.988480	-0.047354	3.272628
239.209937	3562.075620	16.993485	-0.047353	3.269175
239.137102	3554.130574	16.998490	-0.047334	3.265746
239.017928	3546.131650	17.003495	-0.047307	3.262288
238.975861	3538.153702	17.008499	-0.047294	3.258838
238.952645	3530.163743	17.013504	-0.047285	3.255381
238.753252	3522.164623	17.018509	-0.047243	3.251909
238.869605	3514.164488	17.023514	-0.047259	3.248445
238.777477	3506.155416	17.028519	-0.047237	3.244965
238.714814	3498.223354	17.033523	-0.047221	3.241516
238.869205	3490.223688	17.038528	-0.047244	3.238043
238.813271	3482.240607	17.043533	-0.047229	3.234565
238.613037	3474.182224	17.048538	-0.047186	3.231044
238.483726	3466.160431	17.053543	-0.047157	3.227538
238.655999	3458.201368	17.058547	-0.047184	3.224068
238.455763	3450.248586	17.063552	-0.047142	3.220582
238.430130	3442.268169	17.068557	-0.047132	3.217088
238.472806	3434.285030	17.073562	-0.047135	3.213591
238.387782	3426.267127	17.078567	-0.047114	3.210069
238.369248	3418.302224	17.083571	-0.047106	3.206570
238.222084	3410.313496	17.088576	-0.047074	3.203051
238.259939	3402.323164	17.093581	-0.047076	3.199536
238.082224	3394.395362	17.098586	-0.047038	3.196035
238.162686	3386.320199	17.103591	-0.047047	3.192476
238.150920	3378.352528	17.108595	-0.047040	3.188956
238.102143	3370.337921	17.113600	-0.047026	3.185411
238.033340	3362.386347	17.118605	-0.047008	3.181888
238.177081	3354.397862	17.123610	-0.047030	3.178354
237.955379	3346.410442	17.128615	-0.046984	3.174801
237.930265	3338.416639	17.133619	-0.046974	3.171250
237.803336	3330.440236	17.138624	-0.046945	3.167698
237.810000	3322.438886	17.143629	-0.046942	3.164137
237.773436	3314.482945	17.148634	-0.046930	3.160590
237.511080	3306.523622	17.153639	-0.046876	3.157028
237.595536	3298.482367	17.158643	-0.046887	3.153440
237.686322	3290.451699	17.163648	-0.046899	3.149853
237.465283	3282.476645	17.168653	-0.046852	3.146273
237.408100	3274.513531	17.173658	-0.046837	3.142702
237.556085	3266.487907	17.178663	-0.046859	3.139108
237.574429	3258.540414	17.183667	-0.046858	3.135539
237.345217	3250.557659	17.188672	-0.046810	3.131939
237.403551	3242.562056	17.193677	-0.046816	3.128342
237.491539	3234.574767	17.198682	-0.046827	3.124745
237.388866	3226.621746	17.203687	-0.046803	3.121152
237.312260	3218.653940	17.208691	-0.046784	3.117549
237.299057	3210.647689	17.213696	-0.046776	3.113927
237.151398	3202.613174	17.218701	-0.046744	3.110282
237.035857	3194.684050	17.223706	-0.046717	3.106682
237.094152	3186.662232	17.228711	-0.046723	3.103044
237.055495	3178.682858	17.233715	-0.046711	3.099416
236.738134	3170.742899	17.238720	-0.046647	3.095789
236.980306	3162.671159	17.243725	-0.046687	3.092124
237.056404	3154.720033	17.248730	-0.046696	3.088501
236.948974	3146.703798	17.253735	-0.046671	3.084836
236.818488	3138.792991	17.258739	-0.046642	3.081214
236.753124	3130.801775	17.263744	-0.046624	3.077554
236.710778	3122.798696	17.268749	-0.046612	3.073885
236.700167	3114.725791	17.273754	-0.046605	3.070181
236.575577	3106.746945	17.278759	-0.046576	3.066510
236.747612	3098.773871	17.283763	-0.046603	3.062852
236.468871	3090.817755	17.288768	-0.046546	3.059176
236.387463	3082.829447	17.293773	-0.046526	3.055490
236.440445	3074.851210	17.298778	-0.046531	3.051810
236.267871	3066.869328	17.303783	-0.046494	3.048114
236.305869	3058.890336	17.308787	-0.046496	3.044424
236.321384	3050.942857	17.313792	-0.046494	3.040743
236.267685	3042.949591	17.318797	-0.046479	3.037034
236.335805	3034.957517	17.323802	-0.046487	3.033326
236.280610	3026.920212	17.328807	-0.046471	3.029587
236.385048	3018.956006	17.333811	-0.046486	3.025885
236.025939	3011.012351	17.338816	-0.046414	3.022165
235.999408	3003.011816	17.343821	-0.046404	3.018431
235.945709	2995.056096	17.348826	-0.046389	3.014711
235.832928	2987.027044	17.353831	-0.046363	3.010950
236.025345	2979.031307	17.358835	-0.046394	3.007214
235.959355	2971.061963	17.363840	-0.046376	3.003474
235.868969	2963.093858	17.368845	-0.046354	2.999728
235.859124	2955.153791	17.373850	-0.046348	2.995995
235.848777	2947.095093	17.378855	-0.046341	2.992201
235.842635	2939.137529	17.383859	-0.046335	2.988450
235.617656	2931.143124	17.388864	-0.046288	2.984666
235.487510	2923.195105	17.393869	-0.046258	2.980904
235.415159	2915.239155	17.398874	-0.046240	2.977137
235.365239	2907.229008	17.403879	-0.046226	2.973340
235.292926	2899.224939	17.408883	-0.046207	2.969540
235.222501	2891.250002	17.413888	-0.046189	2.965749
235.475364	2883.237461	17.418893	-0.046231	2.961951
235.293751	2875.315878	17.423898	-0.046192	2.958170
235.256016	2867.305248	17.428903	-0.046180	2.954349
235.223249	2859.312307	17.433907	-0.046169	2.950532
235.212833	2851.318173	17.438912	-0.046162	2.946710
235.137677	2843.340126	17.443917	-0.046143	2.942888
235.290594	2835.357494	17.448922	-0.046167	2.939070
235.175381	2827.387001	17.453927	-0.046140	2.935240
235.164767	2819.419477	17.458931	-0.046133	2.931411
235.118415	2811.415687	17.463936	-0.046119	2.927558
234.875053	2803.456301	17.468941	-0.046069	2.923711
234.792350	2795.501569	17.473946	-0.046049	2.919869
234.667828	2787.510910	17.478951	-0.046021	2.916003
234.807067	2779.469032	17.483955	-0.046041	2.912120
234.479874	2771.478846	17.488960	-0.045975	2.908233
234.357561	2763.500726	17.493965	-0.045948	2.904358
234.581164	2755.547144	17.498970	-0.045984	2.900507
234.451428	2747.549434	17.503975	-0.045955	2.896611
234.546859	2739.561297	17.508979	-0.045968	2.892727
234.391325	2731.583556	17.513984	-0.045934	2.888829
234.174110	2723.624167	17.518989	-0.045888	2.884931
234.334626	2715.663549	17.523994	-0.045913	2.881048
234.227384	2707.683564	17.528999	-0.045888	2.877135
234.289767	2699.691068	17.534003	-0.045895	2.873221
234.083767	2691.708352	17.539008	-0.045852	2.869291
234.234092	2683.695432	17.544013	-0.045875	2.865360
234.292842	2675.753154	17.549018	-0.045881	2.861454
234.078311	2667.767647	17.554023	-0.045836	2.857506
233.974681	2659.818707	17.559027	-0.045811	2.853576
233.906386	2651.789046	17.564032	-0.045794	2.849604
233.993540	2643.807861	17.569037	-0.045805	2.845658
233.932010	2635.881619	17.574042	-0.045788	2.841726
233.659707	2627.904833	17.579047	-0.045733	2.837751
233.876759	2619.914460	17.584051	-0.045768	2.833792
233.824685	2611.898735	17.589056	-0.045753	2.829799
233.596589	2603.926335	17.594061	-0.045706	2.825812
233.793382	2595.930480	17.599066	-0.045737	2.821832
233.629525	2587.973371	17.604071	-0.045702	2.817846
233.558424	2580.004506	17.609075	-0.045684	2.813853
233.499518	2572.009492	17.614080	-0.045668	2.809841
233.365619	2564.048231	17.619085	-0.045638	2.805837
233.373412	2556.098825	17.624090	-0.045634	2.801841
233.434674	2548.090132	17.629095	-0.045641	2.797813
233.410889	2540.120721	17.634099	-0.045631	2.793794
233.348815	2532.110381	17.639104	-0.045615	2.789746
233.161635	2524.147199	17.644109	-0.045575	2.785708
233.137882	2516.198843	17.649114	-0.045565	2.781682
233.078714	2508.218760	17.654119	-0.045549	2.777632
233.084738	2500.243357	17.659123	-0.045545	2.773582
232.972251	2492.249893	17.664128	-0.045519	2.769510
232.935643	2484.276516	17.669133	-0.045508	2.765447
232.925632	2476.331329	17.674138	-0.045501	2.761394
232.740048	2468.368960	17.679143	-0.045461	2.757315
233.026553	2460.325755	17.684147	-0.045509	2.753217
232.993161	2452.294295	17.689152	-0.045498	2.749100
232.833590	2444.332330	17.694157	-0.045463	2.745005
232.916630	2436.388870	17.699162	-0.045474	2.740928
232.779485	2428.442026	17.704167	-0.045443	2.736830
232.513547	2420.480671	17.709171	-0.045389	2.732710
232.499967	2412.477325	17.714176	-0.045381	2.728578
232.540588	2404.482677	17.719181	-0.045384	2.724447
232.649903	2396.539541	17.724186	-0.045399	2.720341
232.329086	2388.613946	17.729191	-0.045335	2.716211
232.404831	2380.591313	17.734195	-0.045344	2.712049
232.439370	2372.597878	17.739200	-0.045345	2.707894
232.161294	2364.646396	17.744205	-0.045288	2.703734
232.089008	2356.701721	17.749210	-0.045270	2.699584
232.171504	2348.704115	17.754215	-0.045280	2.695410
232.023678	2340.732297	17.759219	-0.045248	2.691228
231.969778	2332.759233	17.764224	-0.045233	2.687046
232.096383	2324.756590	17.769229	-0.045251	2.682852
232.006287	2316.840675	17.774234	-0.045229	2.678684
231.938348	2308.851517	17.779239	-0.045212	2.674472
231.979383	2300.843411	17.784243	-0.045214	2.670250
232.100884	2292.847009	17.789248	-0.045232	2.666034
231.900983	2284.902937	17.794253	-0.045190	2.661817
231.800950	2276.951726	17.799258	-0.045166	2.657596
231.802535	2268.957294	17.804263	-0.045161	2.653353
231.832042	2260.964015	17.809267	-0.045162	2.649104
231.647135	2253.025351	17.814272	-0.045122	2.644865
231.452519	2245.076151	17.819277	-0.045081	2.640612
231.547076	2237.105464	17.824282	-0.045094	2.636359
231.559919	2229.105474	17.829287	-0.045091	2.632079
231.527703	2221.119681	17.834291	-0.045080	2.627796
231.565306	2213.163857	17.839296	-0.045082	2.623528
231.510336	2205.197030	17.844301	-0.045067	2.619240
231.521020	2197.237455	17.849306	-0.045064	2.614953
231.366211	2189.247581	17.854311	-0.045030	2.610632
231.335082	2181.302974	17.859315	-0.045019	2.606336
231.393680	2173.329185	17.864320	-0.045025	2.602024
231.307503	2165.378869	17.869325	-0.045004	2.597707
231.238646	2157.360104	17.874330	-0.044986	2.593347
230.861694	2149.267562	17.879335	-0.044911	2.588919
230.846820	2141.319716	17.884339	-0.044903	2.584587
230.982446	2133.389453	17.889344	-0.044923	2.580267
230.736134	2125.457074	17.894349	-0.044873	2.575912
230.697894	2117.508353	17.899354	-0.044861	2.571556
230.676709	2109.514686	17.904359	-0.044852	2.567169
230.775916	2101.555527	17.909363	-0.044865	2.562801
230.707376	2093.610973	17.914368	-0.044847	2.558422
230.511146	2085.666252	17.919373	-0.044806	2.554027
230.702525	2077.652835	17.924378	-0.044836	2.549614
230.577872	2069.692197	17.929383	-0.044808	2.545200
230.415191	2061.773066	17.934387	-0.044773	2.540798
230.591877	2053.780972	17.939392	-0.044801	2.536372
230.610576	2045.791758	17.944397	-0.044799	2.531929
230.351426	2037.867177	17.949402	-0.044746	2.527494
230.299218	2029.897200	17.954407	-0.044731	2.523041
230.338989	2021.943191	17.959411	-0.044734	2.518596
230.245286	2013.987206	17.964416	-0.044711	2.514132
230.255970	2005.952782	17.969421	-0.044708	2.509624
230.327018	1997.992413	17.974426	-0.044716	2.505153
230.119713	1990.053307	17.979431	-0.044673	2.500666
230.212888	1982.095839	17.984435	-0.044685	2.496183
229.900193	1974.154895	17.989440	-0.044622	2.491671
229.901721	1966.154214	17.994445	-0.044617	2.487140
229.730354	1958.224073	17.999450	-0.044580	2.482628
229.779595	1950.236702	18.004455	-0.044584	2.478092
229.710996	1942.286375	18.009459	-0.044567	2.473560
229.658216	1934.315241	18.014464	-0.044552	2.469009
229.652770	1926.330822	18.019469	-0.044546	2.464445
229.592758	1918.412444	18.024474	-0.044530	2.459907
229.496729	1910.432410	18.029479	-0.044507	2.455322
229.516500	1902.459208	18.034483	-0.044505	2.450741
229.589615	1894.491995	18.039488	-0.044514	2.446159
229.630577	1886.519552	18.044493	-0.044517	2.441563
229.348735	1878.625907	18.049498	-0.044459	2.436979
229.384526	1870.603868	18.054503	-0.044461	2.432336
229.370421	1862.601014	18.059507	-0.044453	2.427692
229.299769	1854.653683	18.064512	-0.044435	2.423067
229.102318	1846.720951	18.069517	-0.044393	2.418432
229.070597	1838.781028	18.074522	-0.044382	2.413796
229.181123	1830.776392	18.079527	-0.044398	2.409125
229.151053	1822.821344	18.084531	-0.044387	2.404463
229.082808	1814.897182	18.089536	-0.044370	2.399807
229.076568	1806.945158	18.094541	-0.044364	2.395130
228.798001	1798.999254	18.099546	-0.044307	2.390426
228.851255	1790.995447	18.104551	-0.044312	2.385705
229.017025	1783.038235	18.109555	-0.044337	2.381011
228.886801	1775.104738	18.114560	-0.044308	2.376298
228.547981	1767.157840	18.119565	-0.044240	2.371552
228.691985	1759.191708	18.124570	-0.044262	2.366823
228.509804	1751.245334	18.129575	-0.044223	2.362070
228.418826	1743.319197	18.134579	-0.044201	2.357327
228.372551	1735.353273	18.139584	-0.044188	2.352554
228.240819	1727.356873	18.144589	-0.044158	2.347746
228.273265	1719.399557	18.149594	-0.044159	2.342965
228.189041	1711.452797	18.154599	-0.044138	2.338171
228.083397	1703.517798	18.159603	-0.044114	2.333373
228.209532	1695.514528	18.164608	-0.044132	2.328542
228.052233	1687.577203	18.169613	-0.044098	2.323718
228.034531	1679.658967	18.174618	-0.044090	2.318907
227.987627	1671.693006	18.179623	-0.044076	2.314055
227.839782	1663.726908	18.184627	-0.044043	2.309184
227.882248	1655.766165	18.189632	-0.044046	2.304322
227.881393	1647.817691	18.194637	-0.044041	2.299453
227.839559	1639.900054	18.199642	-0.044028	2.294590
227.561556	1631.935142	18.204647	-0.043972	2.289667
227.805702	1623.935806	18.209651	-0.044012	2.284756
227.817014	1616.028785	18.214656	-0.044009	2.279873
227.499941	1608.118838	18.219661	-0.043945	2.274948
227.503809	1600.070722	18.224666	-0.043941	2.269955
227.294458	1592.132035	18.229671	-0.043897	2.265001
227.438607	1584.184558	18.234675	-0.043919	2.260060
227.323990	1576.253357	18.239680	-0.043892	2.255097
227.311532	1568.273649	18.244685	-0.043885	2.250101
227.375921	1560.337238	18.249690	-0.043892	2.245128
227.217536	1552.425632	18.254695	-0.043858	2.240140
227.224947	1544.480611	18.259699	-0.043854	2.235135
227.197161	1536.516569	18.264704	-0.043844	2.230102
226.987281	1528.572129	18.269709	-0.043800	2.225055
227.046899	1520.643667	18.274714	-0.043806	2.220031
227.007127	1512.691154	18.279719	-0.043793	2.214971
226.813833	1504.745888	18.284723	-0.043752	2.209890
226.718455	1496.812054	18.289728	-0.043730	2.204813
226.693234	1488.871059	18.294733	-0.043720	2.199727
226.732695	1480.945855	18.299738	-0.043722	2.194644
226.358074	1472.972956	18.304743	-0.043648	2.189482
226.501782	1465.001543	18.309747	-0.043669	2.184355
226.765549	1457.055095	18.314752	-0.043713	2.179244
226.421879	1449.146459	18.319757	-0.043645	2.174089
226.457072	1441.190433	18.324762	-0.043646	2.168926
226.443813	1433.245358	18.329767	-0.043639	2.163754
226.278309	1425.346721	18.334771	-0.043603	2.158585
226.108176	1417.408646	18.339776	-0.043566	2.153378
225.930337	1409.463870	18.344781	-0.043528	2.148152
226.003594	1401.508746	18.349786	-0.043537	2.142931
225.969101	1393.567326	18.354791	-0.043525	2.137696
226.192474	1385.589455	18.359795	-0.043562	2.132448
226.238247	1377.649743	18.364800	-0.043565	2.127196
226.127191	1369.726561	18.369805	-0.043540	2.121927
225.990785	1361.838022	18.374810	-0.043509	2.116665
225.725696	1353.866215	18.379815	-0.043455	2.111322
225.847362	1345.882407	18.384819	-0.043473	2.105995
225.606039	1337.999131	18.389824	-0.043423	2.100687
225.571993	1330.057190	18.394829	-0.043412	2.095346
225.740283	1322.083697	18.399834	-0.043438	2.089990
225.382580	1314.194928	18.404839	-0.043366	2.084625
225.354386	1306.272785	18.409843	-0.043356	2.079257
225.431138	1298.336756	18.414848	-0.043365	2.073875
225.410463	1290.362185	18.419853	-0.043356	2.068444
225.318377	1282.460776	18.424858	-0.043334	2.063041
225.274286	1274.536876	18.429863	-0.043321	2.057614
225.204126	1266.606135	18.434867	-0.043303	2.052164
225.002754	1258.693528	18.439872	-0.043261	2.046700
225.097228	1250.746540	18.444877	-0.043273	2.041227
225.087793	1242.838975	18.449882	-0.043267	2.035756
224.848357	1234.888300	18.454887	-0.043217	2.030217
224.747457	1226.967751	18.459891	-0.043193	2.024697
224.751621	1219.052003	18.464896	-0.043189	2.019177
224.597779	1211.115025	18.469901	-0.043155	2.013611
224.559546	1203.194316	18.474906	-0.043143	2.008052
224.569058	1195.255217	18.479911	-0.043140	2.002470
224.607685	1187.351143	18.484915	-0.043142	1.996900
224.466014	1179.424871	18.489920	-0.043111	1.991280
224.424982	1171.472901	18.494925	-0.043098	1.985637
224.563833	1163.556859	18.499930	-0.043119	1.980021
224.399655	1155.661337	18.504935	-0.043084	1.974373
224.308432	1147.722921	18.509939	-0.043062	1.968685
224.449799	1139.799005	18.514944	-0.043083	1.963016
224.252158	1131.913056	18.519949	-0.043041	1.957322
224.164631	1123.981618	18.524954	-0.043020	1.951589
224.042797	1116.031502	18.529959	-0.042992	1.945823
223.965760	1108.126852	18.534963	-0.042973	1.940077
223.861962	1100.233404	18.539968	-0.042949	1.934320
223.737361	1092.295346	18.544973	-0.042921	1.928510
223.892782	1084.368191	18.549978	-0.042945	1.922722
223.976526	1076.455626	18.554983	-0.042955	1.916919
223.733719	1068.554960	18.559987	-0.042905	1.911071
223.915379	1060.608674	18.564992	-0.042934	1.905219
223.698325	1052.737821	18.569997	-0.042888	1.899360
223.551688	1044.853049	18.575002	-0.042856	1.893480
223.292113	1036.952359	18.580007	-0.042803	1.887557
223.259252	1029.046105	18.585011	-0.042792	1.881637
223.276312	1021.143830	18.590016	-0.042790	1.875707
223.151779	1013.208831	18.595021	-0.042762	1.869717
223.467574	1005.262591	18.600026	-0.042816	1.863751
223.123049	997.403831	18.605031	-0.042747	1.857755
223.166555	989.475612	18.610035	-0.042750	1.851732
223.067972	981.581621	18.615040	-0.042726	1.845698
222.898424	973.708093	18.620045	-0.042690	1.839653
222.948711	965.803626	18.625050	-0.042694	1.833589
222.988805	957.869544	18.630055	-0.042697	1.827481
223.034769	949.957375	18.635059	-0.042700	1.821371
222.838050	942.114948	18.640064	-0.042659	1.815265
222.596682	934.229647	18.645069	-0.042609	1.809099
222.781665	926.299666	18.650074	-0.042638	1.802929
222.723203	918.424974	18.655079	-0.042623	1.796752
222.302949	910.533191	18.660083	-0.042539	1.790496
222.382679	902.607112	18.665088	-0.042549	1.784251
222.346272	894.718643	18.670093	-0.042538	1.778001
222.102545	886.871145	18.675098	-0.042487	1.771735
222.173177	878.939681	18.680103	-0.042495	1.765419
222.248738	871.059664	18.685107	-0.042504	1.759122
222.204820	863.183725	18.690112	-0.042491	1.752791
222.075817	855.283238	18.695117	-0.042462	1.746407
222.027256	847.416451	18.700122	-0.042448	1.740036
221.835213	839.563163	18.705127	-0.042408	1.733635
221.485750	831.707902	18.710131	-0.042338	1.727188
221.709931	823.798764	18.715136	-0.042374	1.720746
221.790871	815.901286	18.720141	-0.042385	1.714272
221.697193	808.013198	18.725146	-0.042362	1.707758
221.589798	800.144226	18.730151	-0.042337	1.701233
221.497394	792.288681	18.735155	-0.042315	1.694696
221.448390	784.406545	18.740160	-0.042301	1.688117
221.201350	776.562280	18.745165	-0.042250	1.681518
221.183564	768.705246	18.750170	-0.042242	1.674912
221.190619	760.809489	18.755175	-0.042238	1.668251
221.258669	752.919876	18.760179	-0.042246	1.661577
221.194404	745.086174	18.765184	-0.042229	1.654906
221.018579	737.217369	18.770189	-0.042191	1.648162
221.001017	729.371275	18.775194	-0.042183	1.641432
220.843016	721.529797	18.780199	-0.042149	1.634658
220.728771	713.604386	18.785203	-0.042123	1.627790
220.948179	705.726719	18.790208	-0.042159	1.620981
220.803462	697.892131	18.795213	-0.042127	1.614129
220.692277	690.050825	18.800218	-0.042101	1.607248
220.582412	682.213889	18.805223	-0.042076	1.600340
220.184079	674.421588	18.810227	-0.041997	1.593401
220.266773	666.531905	18.815232	-0.042007	1.586414
220.285636	658.675739	18.820237	-0.042006	1.579417
220.393598	650.827385	18.825242	-0.042021	1.572408
220.032354	643.014775	18.830247	-0.041949	1.565332
220.202172	635.166069	18.835251	-0.041975	1.558269
220.231711	627.313590	18.840256	-0.041976	1.551149
219.949526	619.488110	18.845261	-0.041918	1.543976
219.794767	611.685866	18.850266	-0.041885	1.536809
219.747132	603.838883	18.855271	-0.041871	1.529583
219.693553	596.006157	18.860275	-0.041856	1.522335
219.732449	588.189776	18.865280	-0.041858	1.515082
219.373406	580.384630	18.870285	-0.041787	1.507743
219.278299	572.575390	18.875290	-0.041764	1.500405
219.254285	564.753920	18.880295	-0.041755	1.493031
219.147367	556.935758	18.885299	-0.041730	1.485610
219.329141	549.114308	18.890304	-0.041759	1.478194
219.049249	541.292264	18.895309	-0.041702	1.470667
218.890753	533.487329	18.900314	-0.041667	1.463137
218.824022	525.684704	18.905319	-0.041650	1.455585
218.809480	517.858993	18.910323	-0.041642	1.447980
218.725777	510.092555	18.915328	-0.041622	1.440381
218.501490	502.319405	18.920333	-0.041575	1.432713
218.451317	494.509299	18.925338	-0.041561	1.424994
218.352052	486.735139	18.930343	-0.041538	1.417262
218.370116	478.927686	18.935347	-0.041536	1.409473
218.530856	471.127505	18.940352	-0.041561	1.401672
218.241492	463.384611	18.945357	-0.041502	1.393810
218.308619	455.578758	18.950362	-0.041510	1.385899
218.159469	447.828354	18.955367	-0.041477	1.377963
218.018489	440.063997	18.960371	-0.041446	1.369968
217.966898	432.306914	18.965376	-0.041432	1.361949
217.673610	424.584826	18.970381	-0.041372	1.353877
217.828430	416.784327	18.975386	-0.041396	1.345752
217.478081	409.085131	18.980391	-0.041326	1.337596
217.511875	401.304356	18.985395	-0.041328	1.329372
217.507508	393.558190	18.990400	-0.041322	1.321126
217.293015	385.808823	18.995405	-0.041277	1.312787
217.263239	377.983057	19.000410	-0.041267	1.304346
217.364569	370.236766	19.005415	-0.041281	1.295960
217.116700	362.547280	19.010419	-0.041230	1.287518
217.113439	354.840387	19.015424	-0.041224	1.279045
216.869765	347.153728	19.020429	-0.041174	1.270494
216.822334	339.443205	19.025434	-0.041160	1.261895
216.647184	331.763101	19.030439	-0.041123	1.253247
216.719982	324.028914	19.035443	-0.041132	1.244526
216.761036	316.344373	19.040448	-0.041135	1.235793
216.487786	308.668216	19.045453	-0.041079	1.226946
216.198957	301.027180	19.050458	-0.041020	1.218073
216.287021	293.317398	19.055463	-0.041032	1.209128
216.161952	285.655217	19.060467	-0.041004	1.200131
216.054120	278.008463	19.065472	-0.040979	1.191087
215.976152	270.340156	19.070477	-0.040960	1.181955
215.756661	262.731359	19.075482	-0.040914	1.172793
215.563315	255.100425	19.080487	-0.040873	1.163538
215.489239	247.457388	19.085491	-0.040855	1.154219
215.553799	239.767518	19.090496	-0.040862	1.144796
215.190404	232.199074	19.095501	-0.040789	1.135354
215.210048	224.561382	19.100506	-0.040788	1.125828
215.382443	216.926810	19.105511	-0.040815	1.116258
215.278756	209.330999	19.110515	-0.040791	1.106595
215.006747	201.790546	19.115520	-0.040736	1.096880
214.989266	194.186920	19.120525	-0.040728	1.087053
214.919770	186.639105	19.125530	-0.040710	1.077197
214.795411	179.073579	19.130535	-0.040682	1.067215
214.637411	171.534842	19.135539	-0.040648	1.057166
214.485802	164.015490	19.140544	-0.040615	1.047049
214.367057	156.492622	19.145549	-0.040589	1.036836
214.206226	148.991697	19.150554	-0.040554	1.026541
214.244597	141.467788	19.155559	-0.040556	1.016157
213.945256	134.007781	19.160563	-0.040496	1.005674
213.665237	126.570508	19.165568	-0.040439	0.995117
213.588319	119.054688	19.170573	-0.040420	0.984385
213.576472	111.593144	19.175578	-0.040413	0.973630
213.333610	104.172061	19.180583	-0.040363	0.962755
213.222852	96.754898	19.185587	-0.040338	0.951796
213.169369	89.336341	19.190592	-0.040323	0.940721
212.976911	81.960626	19.195597	-0.040283	0.929543
212.778758	74.610441	19.200602	-0.040242	0.918266
212.665288	67.242240	19.205607	-0.040216	0.906844
212.495251	60.141077	19.210611	-0.040180	0.895681