Fri Mar 12 11:07:45 2021


Number of Points = 3594

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
6.243784	-0.012269	0.000000	-0.000014	0.719594
6.118639	0.010219	0.005005	0.000009	0.719594
6.304134	-0.019687	0.010010	-0.000025	0.719600
6.104461	0.012827	0.015014	0.000012	0.719594
6.051703	0.024600	0.020019	0.000022	0.719598
6.152627	0.007856	0.025024	0.000003	0.719600
6.127311	0.009397	0.030029	0.000008	0.719594
6.056665	0.026177	0.035034	0.000021	0.719602
6.192146	-0.002502	0.040038	-0.000004	0.719593
6.265877	-0.012187	0.045043	-0.000017	0.719600
5.971184	0.038913	0.050048	0.000037	0.719597
5.770153	0.074163	0.055053	0.000075	0.719596
5.998779	0.036971	0.060058	0.000032	0.719603
5.801884	0.067684	0.065062	0.000069	0.719594
5.951861	0.044896	0.070067	0.000041	0.719601
6.138191	0.010288	0.075072	0.000007	0.719598
6.188483	-0.089831	0.080077	-0.000002	0.719419
6.125620	-0.152403	0.085082	0.000009	0.719273
6.136602	-0.159184	0.090086	0.000007	0.719263
6.113657	-0.151772	0.095091	0.000012	0.719270
5.940270	-0.123501	0.100096	0.000044	0.719264
5.945940	-0.125578	0.105101	0.000043	0.719262
6.232423	-0.180792	0.110106	-0.000010	0.719254
5.940842	-0.279673	0.115110	0.000044	0.718956
5.800776	-0.252272	0.120115	0.000071	0.718961
6.042385	-0.295420	0.125120	0.000026	0.718960
5.895522	-0.270487	0.130125	0.000053	0.718958
5.913329	-0.269701	0.135130	0.000050	0.718965
5.810697	-0.394145	0.140134	0.000069	0.718684
5.985086	-0.445170	0.145139	0.000037	0.718644
5.944290	-0.439760	0.150144	0.000044	0.718640
5.879571	-0.428587	0.155149	0.000057	0.718639
6.044328	-0.530709	0.160154	0.000026	0.718495
5.962127	-0.591164	0.165158	0.000041	0.718347
5.802104	-0.560210	0.170163	0.000071	0.718352
5.897241	-0.576994	0.175168	0.000054	0.718352
5.857986	-0.694708	0.180173	0.000061	0.718105
5.770571	-0.722038	0.185178	0.000078	0.718020
5.760053	-0.725772	0.190182	0.000080	0.718009
5.942073	-0.790383	0.195187	0.000046	0.717945
5.722004	-0.876333	0.200192	0.000087	0.717698
5.819497	-0.894564	0.205197	0.000069	0.717696
6.020516	-0.939014	0.210202	0.000032	0.717679
5.707589	-1.038492	0.215206	0.000090	0.717372
5.624882	-1.021666	0.220211	0.000105	0.717376
5.514299	-1.002756	0.225216	0.000126	0.717374
5.654444	-1.177620	0.230221	0.000100	0.717077
5.517016	-1.148010	0.235226	0.000126	0.717087
5.202395	-1.110784	0.240230	0.000185	0.717050
5.501058	-1.313028	0.245235	0.000129	0.716755
5.589485	-1.329053	0.250240	0.000113	0.716754
5.592356	-1.390244	0.255245	0.000112	0.716634
5.489451	-1.464591	0.260250	0.000132	0.716450
5.621797	-1.492972	0.265254	0.000107	0.716441
5.662419	-1.626945	0.270259	0.000100	0.716189
5.590523	-1.645222	0.275264	0.000113	0.716128
5.520572	-1.685706	0.280269	0.000126	0.716023
5.469304	-1.746761	0.285274	0.000136	0.715883
5.166166	-1.700556	0.290278	0.000193	0.715868
5.322432	-1.891915	0.295283	0.000164	0.715543
5.307277	-1.889095	0.300288	0.000167	0.715543
4.953549	-1.939040	0.305293	0.000233	0.715319
4.851510	-1.963201	0.310298	0.000252	0.715235
5.106173	-2.071991	0.315302	0.000204	0.715109
4.945399	-2.145464	0.320307	0.000234	0.714906
4.835869	-2.147658	0.325312	0.000255	0.714863
4.190352	-2.164261	0.330317	0.000375	0.714602
3.832451	-2.095976	0.335322	0.000442	0.714611
3.784651	-2.210408	0.340326	0.000451	0.714366
2.909915	-2.100738	0.345331	0.000614	0.714274
2.804794	-2.082675	0.350336	0.000633	0.714273
2.408782	-2.167334	0.355341	0.000707	0.713964
2.271912	-2.138037	0.360346	0.000733	0.713974
1.768557	-2.052636	0.365350	0.000827	0.713965
1.621791	-2.178921	0.370355	0.000854	0.713662
1.484990	-2.158078	0.375360	0.000880	0.713655
0.749738	-2.029041	0.380365	0.001017	0.713651
0.980033	-2.160076	0.385370	0.000974	0.713472
0.135510	-2.067216	0.390374	0.001131	0.713357
0.096769	-2.058466	0.395379	0.001138	0.713361
0.134097	-2.065389	0.400384	0.001132	0.713360
-0.138505	-2.157389	0.405389	0.001183	0.713080
-0.813552	-2.062331	0.410394	0.001308	0.713030
-1.003784	-2.034278	0.415398	0.001344	0.713018
-0.607076	-2.102173	0.420403	0.001270	0.713023
-0.561397	-2.197136	0.425408	0.001262	0.712850
-1.956044	-2.021447	0.430413	0.001521	0.712705
-1.476235	-2.104348	0.435418	0.001432	0.712710
-1.383706	-2.125458	0.440422	0.001415	0.712701
-1.710208	-2.062967	0.445427	0.001476	0.712709
-2.347867	-2.106320	0.450432	0.001595	0.712397
-2.652116	-2.060687	0.455437	0.001651	0.712379
-2.538323	-2.075513	0.460442	0.001630	0.712390
-2.556048	-2.078622	0.465446	0.001634	0.712377
-2.496644	-2.084815	0.470451	0.001623	0.712386
-2.754791	-2.140171	0.475456	0.001671	0.712184
-3.697144	-2.023215	0.480461	0.001846	0.712082
-3.261241	-2.095714	0.485466	0.001765	0.712092
-3.400732	-2.075439	0.490470	0.001791	0.712083
-3.524392	-2.051482	0.495475	0.001814	0.712087
-3.461902	-2.072954	0.500480	0.001803	0.712066
-4.149970	-2.105096	0.505485	0.001931	0.711757
-3.987297	-2.130243	0.510490	0.001901	0.711765
-4.561911	-2.032078	0.515494	0.002008	0.711756
-4.147443	-2.103110	0.520499	0.001931	0.711762
-4.001253	-2.130840	0.525504	0.001904	0.711758
-4.603669	-2.065496	0.530509	0.002016	0.711674
-5.309394	-2.051123	0.535514	0.002147	0.711452
-5.046405	-2.099470	0.540518	0.002099	0.711449
-5.061863	-2.095304	0.545523	0.002102	0.711452
-4.975721	-2.110690	0.550528	0.002086	0.711451
-5.074032	-2.094930	0.555533	0.002104	0.711448
-5.085059	-2.109396	0.560538	0.002106	0.711415
-6.018554	-2.084001	0.565542	0.002280	0.711133
-6.125571	-2.064028	0.570547	0.002300	0.711135
-6.221799	-2.045782	0.575552	0.002318	0.711137
-6.176967	-2.056701	0.580557	0.002310	0.711131
-6.051826	-2.074539	0.585562	0.002287	0.711140
-6.020326	-2.084608	0.590566	0.002281	0.711131
-5.981263	-2.163291	0.595571	0.002274	0.710987
-6.719038	-2.090977	0.600576	0.002411	0.710869
-6.898749	-2.061568	0.605581	0.002445	0.710864
-6.679427	-2.095840	0.610586	0.002404	0.710873
-6.943220	-2.051057	0.615590	0.002453	0.710869
-6.592206	-2.113058	0.620595	0.002388	0.710870
-6.496003	-2.183875	0.625600	0.002370	0.710762
-7.933967	-2.045344	0.630605	0.002638	0.710527
-7.774187	-2.068422	0.635610	0.002608	0.710538
-8.046460	-2.024040	0.640614	0.002659	0.710529
-7.897298	-2.048626	0.645619	0.002631	0.710533
-7.852915	-2.054930	0.650624	0.002623	0.710536
-7.982365	-2.036626	0.655629	0.002647	0.710526
-7.896028	-2.106556	0.660634	0.002631	0.710417
-8.831178	-2.043581	0.665638	0.002805	0.710210
-8.689439	-2.067431	0.670643	0.002779	0.710213
-8.942680	-2.020072	0.675648	0.002826	0.710217
-8.917019	-2.028274	0.680653	0.002822	0.710210
-8.748101	-2.054351	0.685658	0.002790	0.710217
-8.760114	-2.056659	0.690662	0.002793	0.710208
-8.573601	-2.132428	0.695667	0.002758	0.710123
-9.544206	-2.076321	0.700672	0.002939	0.709889
-9.445414	-2.096813	0.705677	0.002921	0.709884
-9.452590	-2.089987	0.710682	0.002922	0.709894
-9.623459	-2.065233	0.715686	0.002954	0.709883
-9.676771	-2.052488	0.720691	0.002964	0.709889
-9.176838	-2.141073	0.725696	0.002871	0.709890
-9.522495	-2.168900	0.730701	0.002935	0.709711
-10.496349	-2.052008	0.735706	0.003117	0.709598
-10.554001	-2.047272	0.740710	0.003127	0.709586
-10.401182	-2.071382	0.745715	0.003099	0.709592
-10.443841	-2.063269	0.750720	0.003107	0.709593
-10.562465	-2.044973	0.755725	0.003129	0.709587
-10.254404	-2.096477	0.760730	0.003072	0.709594
-10.650933	-2.139190	0.765734	0.003146	0.709367
-11.976189	-1.956439	0.770739	0.003393	0.709260
-11.217433	-2.088971	0.775744	0.003252	0.709265
-11.313737	-2.075081	0.780749	0.003270	0.709259
-11.566378	-2.024981	0.785754	0.003317	0.709269
-11.539139	-2.035683	0.790758	0.003312	0.709257
-11.357385	-2.067253	0.795763	0.003278	0.709258
-11.252442	-2.137981	0.800768	0.003259	0.709154
-12.719161	-1.978968	0.805773	0.003532	0.708949
-12.026001	-2.098877	0.810778	0.003403	0.708956
-12.519398	-2.013277	0.815782	0.003495	0.708951
-12.506392	-2.015514	0.820787	0.003492	0.708951
-11.902674	-2.121822	0.825792	0.003380	0.708953
-12.446831	-2.026863	0.830797	0.003481	0.708949
-12.457651	-2.034912	0.835802	0.003484	0.708929
-13.120252	-2.065785	0.840806	0.003607	0.708631
-12.974022	-2.089233	0.845811	0.003580	0.708636
-13.192937	-2.049122	0.850816	0.003621	0.708638
-13.434769	-2.010147	0.855821	0.003666	0.708629
-13.129823	-2.059467	0.860826	0.003609	0.708639
-13.078095	-2.071372	0.865830	0.003600	0.708634
-13.306667	-2.029501	0.870835	0.003642	0.708636
-13.626221	-2.101427	0.875840	0.003702	0.708377
-14.268735	-2.003773	0.880845	0.003822	0.708344
-13.954592	-2.056527	0.885850	0.003763	0.708350
-13.977490	-2.055364	0.890854	0.003768	0.708344
-14.067899	-2.037611	0.895859	0.003784	0.708347
-13.925075	-2.060999	0.900864	0.003758	0.708351
-14.222348	-2.011011	0.905869	0.003813	0.708345
-14.288056	-2.147437	0.910874	0.003826	0.708048
-14.746901	-2.084456	0.915878	0.003911	0.708010
-15.135509	-2.015499	0.920883	0.003984	0.708009
-14.658245	-2.099900	0.925888	0.003895	0.708010
-14.753295	-2.085019	0.930893	0.003913	0.708006
-15.042517	-2.029066	0.935898	0.003967	0.708015
-15.162666	-2.016446	0.940902	0.003989	0.707997
-15.379963	-2.128267	0.945907	0.004030	0.707695
-15.459057	-2.112531	0.950912	0.004044	0.707698
-16.292234	-1.968691	0.955917	0.004200	0.707688
-15.767993	-2.056214	0.960922	0.004102	0.707700
-15.638576	-2.083403	0.965926	0.004078	0.707692
-15.937802	-2.029442	0.970931	0.004134	0.707693
-15.759447	-2.072903	0.975936	0.004101	0.707669
-16.596228	-2.073881	0.980941	0.004257	0.707368
-16.657864	-2.059118	0.985946	0.004268	0.707375
-16.988387	-2.002535	0.990950	0.004330	0.707370
-16.588389	-2.072895	0.995955	0.004255	0.707372
-16.447344	-2.095893	1.000960	0.004229	0.707376
-16.924898	-2.014969	1.005965	0.004318	0.707368
-16.725614	-2.046441	1.010970	0.004281	0.707376
-16.819622	-2.161591	1.015974	0.004299	0.707111
-17.779926	-2.007911	1.020979	0.004478	0.707075
-17.578275	-2.041014	1.025984	0.004440	0.707081
-17.347485	-2.087163	1.030989	0.004397	0.707071
-17.635878	-2.030311	1.035994	0.004451	0.707082
-17.861325	-1.993660	1.040998	0.004493	0.707074
-17.711244	-2.020486	1.046003	0.004465	0.707074
-17.629925	-2.167917	1.051008	0.004450	0.706807
-18.798176	-1.991420	1.056013	0.004668	0.706743
-18.522265	-2.035080	1.061018	0.004617	0.706754
-18.259030	-2.086468	1.066022	0.004568	0.706745
-18.361665	-2.067509	1.071027	0.004587	0.706746
-18.406584	-2.056584	1.076032	0.004595	0.706752
-18.419354	-2.058695	1.081037	0.004598	0.706743
-18.770954	-2.136310	1.086042	0.004663	0.706461
-19.547709	-2.009653	1.091046	0.004808	0.706437
-19.592885	-2.000937	1.096051	0.004817	0.706438
-18.954898	-2.112677	1.101056	0.004698	0.706442
-19.401641	-2.036923	1.106061	0.004781	0.706434
-19.240328	-2.060936	1.111066	0.004751	0.706443
-19.163263	-2.080224	1.116070	0.004737	0.706432
-20.171057	-2.054583	1.121075	0.004925	0.706122
-20.471309	-1.999310	1.126080	0.004981	0.706125
-20.683501	-1.965751	1.131085	0.005020	0.706117
-20.085811	-2.067983	1.136090	0.004909	0.706125
-20.511975	-1.994107	1.141094	0.004988	0.706121
-20.674009	-1.963861	1.146099	0.005019	0.706123
-19.926604	-2.096197	1.151104	0.004880	0.706125
-20.445340	-2.057800	1.156109	0.004976	0.706016
-21.350008	-1.975085	1.161114	0.005145	0.705858
-21.021029	-2.035784	1.166118	0.005084	0.705854
-21.085359	-2.024196	1.171123	0.005096	0.705854
-21.043481	-2.029562	1.176128	0.005088	0.705858
-21.049749	-2.032089	1.181133	0.005089	0.705850
-20.973001	-2.041342	1.186138	0.005075	0.705859
-21.274951	-2.066982	1.191142	0.005131	0.705699
-22.167289	-1.999419	1.196147	0.005298	0.705515
-21.698308	-2.080925	1.201152	0.005210	0.705519
-22.108837	-2.011888	1.206157	0.005287	0.705510
-22.158927	-1.997253	1.211162	0.005296	0.705522
-21.628485	-2.094447	1.216166	0.005198	0.705516
-21.852899	-2.054399	1.221171	0.005240	0.705516
-22.292515	-2.072363	1.226176	0.005321	0.705322
-23.216270	-1.968711	1.231181	0.005493	0.705199
-22.652424	-2.062595	1.236186	0.005389	0.705212
-23.051437	-1.994328	1.241190	0.005463	0.705206
-23.358605	-1.941077	1.246195	0.005520	0.705203
-22.788879	-2.039150	1.251200	0.005414	0.705210
-23.075117	-1.992576	1.256205	0.005468	0.705201
-23.186141	-1.998290	1.261210	0.005488	0.705149
-23.618130	-2.055771	1.266214	0.005569	0.704878
-23.703306	-2.039187	1.271219	0.005585	0.704881
-23.995975	-1.984334	1.276224	0.005639	0.704886
-23.967443	-1.993950	1.281229	0.005634	0.704877
-23.626673	-2.050396	1.286234	0.005571	0.704886
-23.872393	-2.008291	1.291238	0.005617	0.704882
-24.019859	-1.988780	1.296243	0.005644	0.704868
-24.283246	-2.082303	1.301248	0.005693	0.704585
-24.854233	-1.981627	1.306253	0.005800	0.704583
-25.164707	-1.921275	1.311258	0.005858	0.704593
-24.582289	-2.029443	1.316262	0.005749	0.704584
-24.827866	-1.987091	1.321267	0.005795	0.704581
-25.033571	-1.946967	1.326272	0.005833	0.704587
-25.045094	-1.949673	1.331277	0.005836	0.704578
-24.584668	-2.121723	1.336282	0.005750	0.704396
-25.942697	-1.950503	1.341286	0.006003	0.704253
-25.987112	-1.943239	1.346291	0.006011	0.704252
-25.368798	-2.050683	1.351296	0.005896	0.704257
-25.490797	-2.033574	1.356301	0.005919	0.704248
-25.639959	-2.000938	1.361306	0.005947	0.704260
-25.723209	-1.990854	1.366310	0.005963	0.704250
-25.541071	-2.106938	1.371315	0.005929	0.704081
-26.494793	-2.001571	1.376320	0.006106	0.703950
-26.647093	-1.979096	1.381325	0.006135	0.703941
-26.528856	-1.997850	1.386330	0.006113	0.703945
-26.642527	-1.978780	1.391334	0.006134	0.703943
-26.837398	-1.945465	1.396339	0.006171	0.703940
-26.276717	-2.040857	1.401344	0.006066	0.703949
-26.455188	-2.091800	1.406349	0.006100	0.703782
-27.578953	-1.965057	1.411354	0.006309	0.703633
-27.102352	-2.052850	1.416358	0.006220	0.703627
-27.001567	-2.070622	1.421363	0.006202	0.703627
-27.199623	-2.032947	1.426368	0.006239	0.703632
-27.510402	-1.982639	1.431373	0.006296	0.703622
-26.984620	-2.072510	1.436378	0.006199	0.703629
-27.500855	-2.120033	1.441382	0.006295	0.703347
-28.147493	-2.012740	1.446387	0.006415	0.703331
-28.135620	-2.010485	1.451392	0.006413	0.703340
-27.792949	-2.076565	1.456397	0.006350	0.703330
-28.031974	-2.030155	1.461402	0.006394	0.703337
-28.288555	-1.985757	1.466406	0.006442	0.703334
-28.063120	-2.105700	1.471411	0.006400	0.703173
-28.884755	-2.042876	1.476416	0.006553	0.703004
-29.247621	-1.982849	1.481421	0.006621	0.702994
-29.035783	-2.015823	1.486426	0.006581	0.703004
-28.903366	-2.042830	1.491430	0.006557	0.702997
-29.170893	-1.996169	1.496435	0.006607	0.702994
-29.043148	-2.014073	1.501440	0.006583	0.703004
-29.041630	-2.082772	1.506445	0.006583	0.702866
-30.213716	-1.960355	1.511450	0.006801	0.702691
-29.987962	-2.002033	1.516454	0.006759	0.702688
-29.904466	-2.017380	1.521459	0.006744	0.702687
-29.936742	-2.007835	1.526464	0.006750	0.702694
-30.317505	-1.945773	1.531469	0.006821	0.702682
-29.982588	-2.000000	1.536474	0.006759	0.702693
-29.723205	-2.071969	1.541478	0.006710	0.702641
-30.959017	-1.988235	1.546483	0.006941	0.702365
-30.944707	-1.988736	1.551488	0.006938	0.702369
-31.004284	-1.981352	1.556493	0.006949	0.702362
-30.591279	-2.052518	1.561498	0.006872	0.702367
-30.925424	-1.993861	1.566502	0.006935	0.702365
-30.864636	-2.007205	1.571507	0.006923	0.702359
-30.580192	-2.058961	1.576512	0.006871	0.702357
-31.610675	-2.020112	1.581517	0.007062	0.702064
-31.602194	-2.017761	1.586522	0.007061	0.702072
-31.526093	-2.031057	1.591526	0.007047	0.702072
-31.582795	-2.022717	1.596531	0.007058	0.702068
-31.785437	-1.982682	1.601536	0.007095	0.702076
-31.857649	-1.976092	1.606541	0.007109	0.702063
-31.586325	-2.042373	1.611546	0.007058	0.702027
-32.549608	-2.013193	1.616550	0.007238	0.701738
-32.549654	-2.013953	1.621555	0.007238	0.701736
-32.571069	-2.004190	1.626560	0.007242	0.701748
-33.014346	-1.930543	1.631565	0.007325	0.701737
-32.861313	-1.954317	1.636570	0.007296	0.701744
-32.461524	-2.026835	1.641574	0.007222	0.701742
-32.914395	-1.946926	1.646579	0.007306	0.701740
-33.052595	-2.016764	1.651584	0.007332	0.701548
-33.730986	-1.953472	1.656589	0.007459	0.701431
-33.338707	-2.020990	1.661594	0.007386	0.701436
-33.812941	-1.939659	1.666598	0.007474	0.701429
-33.857843	-1.929720	1.671603	0.007482	0.701433
-33.057444	-2.068162	1.676608	0.007334	0.701442
-33.292037	-2.030490	1.681613	0.007377	0.701433
-33.817772	-2.026478	1.686618	0.007475	0.701251
-34.480725	-1.973733	1.691622	0.007599	0.701118
-34.075769	-2.047791	1.696627	0.007523	0.701115
-34.006744	-2.055741	1.701632	0.007511	0.701123
-34.258851	-2.015174	1.706637	0.007558	0.701114
-34.038896	-2.051387	1.711642	0.007517	0.701120
-34.172467	-2.041167	1.716646	0.007542	0.701092
-34.791880	-2.042128	1.721651	0.007657	0.700866
-34.269971	-2.130610	1.726656	0.007560	0.700876
-34.855094	-2.031194	1.731661	0.007669	0.700865
-34.916624	-2.016134	1.736666	0.007681	0.700874
-34.519756	-2.088558	1.741670	0.007607	0.700870
-34.703709	-2.096195	1.746675	0.007641	0.700788
-35.879543	-2.010816	1.751680	0.007860	0.700536
-35.613508	-2.063143	1.756685	0.007811	0.700526
-35.389868	-2.098862	1.761690	0.007769	0.700534
-35.628184	-2.057437	1.766694	0.007814	0.700532
-35.870132	-2.015364	1.771699	0.007859	0.700529
-35.780108	-2.028950	1.776704	0.007842	0.700534
-36.207657	-2.091741	1.781709	0.007922	0.700252
-36.709415	-2.019344	1.786714	0.008015	0.700217
-36.715209	-2.020577	1.791718	0.008017	0.700213
-36.487527	-2.062061	1.796723	0.007974	0.700211
-36.454476	-2.063410	1.801728	0.007968	0.700220
-36.903686	-1.989030	1.806733	0.008052	0.700208
-36.416002	-2.110129	1.811738	0.007961	0.700139
-37.317087	-2.073387	1.816742	0.008129	0.699887
-37.611382	-2.021169	1.821747	0.008184	0.699886
-37.451007	-2.046765	1.826752	0.008154	0.699892
-37.548378	-2.032819	1.831757	0.008172	0.699885
-37.587913	-2.021917	1.836762	0.008180	0.699893
-37.568533	-2.028100	1.841766	0.008176	0.699887
-37.599027	-2.074043	1.846771	0.008182	0.699783
-38.206433	-2.056464	1.851776	0.008295	0.699598
-38.345737	-2.036384	1.856781	0.008321	0.699588
-38.243116	-2.050682	1.861786	0.008302	0.699596
-38.247369	-2.050881	1.866790	0.008303	0.699594
-38.466165	-2.013817	1.871795	0.008344	0.699590
-38.257641	-2.045964	1.876800	0.008305	0.699600
-38.305199	-2.149306	1.881805	0.008314	0.699373
-39.299307	-2.024622	1.886810	0.008499	0.699266
-39.398612	-2.006715	1.891814	0.008518	0.699266
-39.306343	-2.025703	1.896819	0.008501	0.699261
-39.312343	-2.022515	1.901824	0.008502	0.699265
-39.470987	-1.998828	1.906829	0.008532	0.699255
-39.240478	-2.035783	1.911834	0.008489	0.699264
-39.255240	-2.128399	1.916838	0.008492	0.699070
-40.502267	-1.962843	1.921843	0.008724	0.698954
-39.900101	-2.067507	1.926848	0.008612	0.698960
-40.022196	-2.050144	1.931853	0.008635	0.698951
-40.253428	-2.004482	1.936858	0.008678	0.698959
-40.167011	-2.022387	1.941862	0.008662	0.698954
-40.032846	-2.046426	1.946867	0.008637	0.698954
-40.273209	-2.125870	1.951872	0.008682	0.698705
-41.459643	-1.947820	1.956877	0.008903	0.698637
-41.273390	-1.979191	1.961882	0.008868	0.698640
-40.714191	-2.079727	1.966886	0.008764	0.698639
-41.346264	-1.968488	1.971891	0.008882	0.698635
-41.029460	-2.021608	1.976896	0.008823	0.698642
-40.982881	-2.035017	1.981901	0.008814	0.698632
-41.129143	-2.090885	1.986906	0.008842	0.698465
-41.896785	-2.009733	1.991910	0.008985	0.698351
-41.679022	-2.050525	1.996915	0.008944	0.698347
-41.743127	-2.036919	2.001920	0.008956	0.698351
-41.606349	-2.060998	2.011917	0.008931	0.698352
-41.727958	-2.084370	2.021914	0.008954	0.698260
-42.935934	-1.991292	2.031910	0.009179	0.698010
-42.805007	-2.015135	2.041907	0.009155	0.698009
-42.711883	-2.028586	2.051904	0.009138	0.698015
-42.113147	-2.047674	2.061901	0.009026	0.698193
-42.282034	-1.984081	2.071898	0.009058	0.698261
-41.868820	-2.041366	2.081894	0.008981	0.698294
-42.007475	-1.989192	2.091891	0.009007	0.698349
-41.603824	-2.061100	2.101888	0.008932	0.698349
-41.737229	-2.036068	2.111885	0.008957	0.698352
-41.821677	-2.020998	2.121882	0.008973	0.698351
-41.802594	-2.024508	2.131878	0.008970	0.698351
-41.938243	-2.001150	2.141875	0.008995	0.698349
-41.682261	-2.023357	2.151872	0.008948	0.698396
-40.943876	-2.033933	2.161869	0.008810	0.698642
-41.041684	-2.018325	2.171866	0.008829	0.698638
-40.980690	-2.029387	2.181862	0.008817	0.698637
-40.993526	-2.027012	2.191859	0.008820	0.698637
-40.501679	-2.010300	2.201856	0.008729	0.698849
-40.133266	-2.023503	2.211853	0.008660	0.698955
-40.123130	-2.024725	2.221850	0.008658	0.698956
-39.905145	-2.063786	2.231846	0.008618	0.698955
-39.696211	-2.010685	2.241843	0.008579	0.699139
-39.202962	-2.036509	2.251840	0.008488	0.699265
-39.082393	-2.057310	2.261837	0.008465	0.699266
-39.165434	-2.043415	2.271834	0.008481	0.699264
-38.793374	-1.989187	2.281830	0.008412	0.699508
-38.496462	-1.998670	2.291827	0.008357	0.699596
-38.221794	-2.047877	2.301824	0.008306	0.699595
-38.186331	-2.047418	2.311821	0.008299	0.699609
-37.665632	-1.999491	2.321818	0.008202	0.699894
-37.595154	-2.012822	2.331814	0.008190	0.699892
-37.675548	-1.997976	2.341811	0.008205	0.699893
-37.186319	-1.988298	2.351808	0.008114	0.700089
-36.925174	-1.971519	2.361805	0.008065	0.700217
-36.793629	-1.993852	2.371802	0.008041	0.700219
-36.818422	-1.936860	2.381798	0.008046	0.700326
-36.160474	-1.952001	2.391795	0.007923	0.700532
-36.070415	-1.968477	2.401792	0.007907	0.700531
-36.111454	-1.929460	2.411789	0.007915	0.700595
-35.366010	-1.925874	2.421786	0.007776	0.700872
-35.172768	-1.959285	2.431782	0.007740	0.700873
-35.254244	-1.946599	2.441779	0.007755	0.700869
-34.641684	-1.939168	2.451776	0.007642	0.701105
-34.364874	-1.981885	2.461773	0.007590	0.701118
-34.472239	-1.962152	2.471770	0.007610	0.701119
-34.208611	-1.899595	2.481766	0.007561	0.701341
-33.835895	-1.921544	2.491763	0.007492	0.701431
-33.556608	-1.970257	2.501760	0.007440	0.701432
-33.166953	-1.964022	2.511757	0.007368	0.701585
-32.780054	-1.957085	2.521754	0.007296	0.701739
-32.699331	-1.971703	2.531750	0.007281	0.701738
-32.622641	-1.971235	2.541747	0.007267	0.701766
-32.011513	-1.929384	2.551744	0.007154	0.702071
-31.810257	-1.964026	2.561741	0.007116	0.702073
-31.855289	-1.956027	2.571738	0.007125	0.702073
-31.428066	-1.929439	2.581734	0.007045	0.702280
-31.116016	-1.943210	2.591731	0.006987	0.702365
-31.283923	-1.912490	2.601728	0.007019	0.702366
-31.017991	-1.875309	2.611725	0.006970	0.702537
-30.678309	-1.858179	2.621722	0.006906	0.702693
-30.729642	-1.851687	2.631718	0.006916	0.702688
-30.348099	-1.820224	2.641715	0.006845	0.702888
-30.014152	-1.820796	2.651712	0.006783	0.703007
-30.168060	-1.794159	2.661709	0.006812	0.703005
-29.879899	-1.706480	2.671706	0.006759	0.703286
-29.709760	-1.710097	2.681702	0.006727	0.703339
-29.384563	-1.729125	2.691699	0.006667	0.703418
-29.047234	-1.682698	2.701696	0.006604	0.703632
-28.767544	-1.731201	2.711693	0.006552	0.703635
-28.554085	-1.670557	2.721690	0.006512	0.703834
-28.215039	-1.673232	2.731686	0.006450	0.703950
-28.148931	-1.684817	2.741683	0.006437	0.703950
-27.793821	-1.598566	2.751680	0.006371	0.704251
-27.486212	-1.648787	2.761677	0.006314	0.704260
-27.225646	-1.646543	2.771674	0.006266	0.704358
-26.719970	-1.622493	2.781670	0.006172	0.704588
-26.442747	-1.671947	2.791667	0.006121	0.704587
-26.201297	-1.667900	2.801664	0.006076	0.704682
-25.730487	-1.650419	2.811661	0.005988	0.704886
-25.642392	-1.665302	2.821658	0.005972	0.704887
-25.522876	-1.657035	2.831654	0.005950	0.704946
-25.070300	-1.607615	2.841651	0.005866	0.705208
-24.723303	-1.670322	2.851648	0.005801	0.705206
-24.568339	-1.694486	2.861645	0.005773	0.705213
-24.248981	-1.596759	2.871642	0.005713	0.705524
-23.971362	-1.647563	2.881638	0.005662	0.705521
-23.703969	-1.696117	2.891635	0.005612	0.705519
-23.447605	-1.619454	2.901632	0.005565	0.705764
-23.229896	-1.611399	2.911629	0.005524	0.705858
-23.003652	-1.651257	2.921626	0.005482	0.705859
-22.736239	-1.639698	2.931622	0.005433	0.705978
-22.452359	-1.617148	2.941619	0.005380	0.706125
-22.506235	-1.606332	2.951616	0.005390	0.706127
-22.209545	-1.605722	2.961613	0.005335	0.706234
-21.781920	-1.579446	2.971610	0.005256	0.706440
-21.482454	-1.633015	2.981606	0.005200	0.706439
-21.196472	-1.670453	2.991603	0.005147	0.706466
-20.921246	-1.578030	3.001600	0.005096	0.706750
-20.688042	-1.619398	3.011597	0.005053	0.706750
-20.582449	-1.640159	3.021594	0.005033	0.706746
-20.394032	-1.537380	3.031590	0.004998	0.707019
-20.071474	-1.566649	3.041587	0.004938	0.707075
-19.822467	-1.610288	3.051584	0.004892	0.707077
-19.359723	-1.591969	3.061581	0.004806	0.707279
-19.207795	-1.573132	3.071578	0.004778	0.707370
-18.962285	-1.617315	3.081574	0.004733	0.707369
-19.012019	-1.542040	3.091571	0.004742	0.707502
-18.515399	-1.535928	3.101568	0.004650	0.707692
-18.455749	-1.545229	3.111565	0.004639	0.707694
-18.359274	-1.497853	3.121562	0.004621	0.707823
-18.017846	-1.467231	3.131558	0.004557	0.708006
-17.707322	-1.523857	3.141555	0.004500	0.708003
-17.526791	-1.475410	3.151552	0.004466	0.708165
-17.192620	-1.446449	3.161549	0.004404	0.708342
-16.990802	-1.481283	3.171546	0.004367	0.708344
-16.880064	-1.417859	3.181542	0.004346	0.708510
-16.664387	-1.393952	3.191539	0.004306	0.708635
-16.555515	-1.412882	3.201536	0.004286	0.708635
-16.222818	-1.335709	3.211533	0.004224	0.708908
-15.836517	-1.381055	3.221530	0.004153	0.708955
-15.720245	-1.385806	3.231526	0.004131	0.708987
-15.259678	-1.331702	3.241523	0.004046	0.709259
-14.904998	-1.393385	3.251520	0.003980	0.709262
-14.715876	-1.400372	3.261517	0.003945	0.709315
-14.325406	-1.329762	3.271514	0.003872	0.709595
-14.171012	-1.358834	3.281510	0.003844	0.709592
-14.129287	-1.342157	3.291507	0.003836	0.709639
-13.571034	-1.315100	3.301504	0.003732	0.709892
-13.189267	-1.382310	3.311501	0.003661	0.709893
-12.997206	-1.417352	3.321498	0.003626	0.709892
-12.814029	-1.290086	3.331494	0.003592	0.710211
-12.750081	-1.299873	3.341491	0.003580	0.710214
-12.540786	-1.334937	3.351488	0.003541	0.710218
-12.297822	-1.220205	3.361485	0.003496	0.710533
-11.977376	-1.276796	3.371482	0.003437	0.710534
-11.838448	-1.278973	3.381478	0.003411	0.710579
-11.533177	-1.188609	3.391475	0.003354	0.710868
-11.195542	-1.248144	3.401472	0.003292	0.710868
-10.843565	-1.287218	3.411469	0.003226	0.710915
-10.459505	-1.243989	3.421466	0.003155	0.711138
-10.267849	-1.278567	3.431462	0.003119	0.711137
-10.067036	-1.315599	3.441459	0.003082	0.711134
-9.925601	-1.182795	3.451456	0.003056	0.711449
-9.615349	-1.235724	3.461453	0.002998	0.711453
-9.066575	-1.333076	3.471450	0.002896	0.711454
-8.897391	-1.239239	3.481446	0.002865	0.711701
-8.517414	-1.279272	3.491443	0.002794	0.711756
-8.459129	-1.288124	3.501440	0.002784	0.711758
-8.204364	-1.260449	3.511437	0.002736	0.711904
-7.956216	-1.211423	3.521434	0.002690	0.712089
-7.650190	-1.268104	3.531430	0.002634	0.712085
-7.637161	-1.237793	3.541427	0.002631	0.712149
-7.391301	-1.163612	3.551424	0.002586	0.712384
-7.248807	-1.187977	3.561421	0.002559	0.712386
-7.147290	-1.162629	3.571418	0.002541	0.712472
-6.926066	-1.087221	3.581414	0.002500	0.712700
-6.648431	-1.135193	3.591411	0.002448	0.712703
-6.544854	-1.062378	3.601408	0.002429	0.712884
-6.422502	-1.015700	3.611405	0.002406	0.713020
-6.319541	-1.018137	3.621402	0.002387	0.713052
-6.046305	-0.915719	3.631398	0.002336	0.713352
-5.714589	-0.975012	3.641395	0.002275	0.713351
-5.446579	-0.926340	3.651392	0.002225	0.713543
-5.193861	-0.918151	3.661389	0.002178	0.713648
-5.127186	-0.892057	3.671386	0.002166	0.713724
-4.939229	-0.804889	3.681382	0.002131	0.713963
-4.730714	-0.843646	3.691379	0.002092	0.713960
-4.120042	-0.803859	3.701376	0.001979	0.714254
-3.633955	-0.879952	3.711373	0.001889	0.714275
-3.437572	-0.867058	3.721370	0.001852	0.714370
-3.080548	-0.812806	3.731366	0.001786	0.714604
-3.027593	-0.823613	3.741363	0.001776	0.714601
-2.884944	-0.761562	3.751360	0.001750	0.714774
-2.846716	-0.703250	3.761357	0.001743	0.714903
-2.564658	-0.721167	3.771354	0.001690	0.714967
-2.362620	-0.626164	3.781350	0.001653	0.715226
-2.365666	-0.625459	3.791347	0.001654	0.715226
-2.061040	-0.530989	3.801344	0.001597	0.715521
-1.806952	-0.565253	3.811341	0.001550	0.715542
-1.462598	-0.503614	3.821338	0.001486	0.715786
-1.151240	-0.511764	3.831334	0.001428	0.715879
-1.065120	-0.475683	3.841331	0.001412	0.715981
-0.976940	-0.419254	3.851328	0.001396	0.716124
-0.949599	-0.368660	3.861325	0.001391	0.716233
-0.784875	-0.292222	3.871322	0.001360	0.716442
-0.730051	-0.237066	3.881318	0.001350	0.716571
-0.687170	-0.153876	3.891315	0.001343	0.716750
-0.413996	-0.101061	3.901312	0.001292	0.716951
-0.289903	-0.057288	3.911309	0.001269	0.717081
-0.022011	0.027095	3.921306	0.001219	0.717342
0.025985	0.067902	3.931302	0.001210	0.717439
0.000000	0.253518	3.941299	0.001215	0.717797
0.063168	0.863736	3.946304	0.001203	0.719024
0.619099	2.021419	3.951309	0.001099	0.721499
1.397145	3.731769	3.956314	0.000953	0.725126
3.050645	5.863712	3.961318	0.000644	0.729858
4.068656	8.632891	3.966323	0.000453	0.735570
5.035266	11.894812	3.971328	0.000270	0.742163
6.091550	15.602227	3.976333	0.000071	0.749572
6.821181	19.779719	3.981338	-0.000067	0.757680
7.575398	24.349819	3.986342	-0.000210	0.766437
8.094218	29.332873	3.991347	-0.000310	0.775773
8.659527	34.644431	3.996352	-0.000419	0.785607
9.255712	40.286110	4.001357	-0.000533	0.795917
9.856622	46.205670	4.006362	-0.000649	0.806585
11.730388	52.209164	4.011366	-0.001002	0.817650
12.750259	58.641415	4.016371	-0.001196	0.829042
13.341193	65.386476	4.021376	-0.001310	0.840679
13.735806	72.375903	4.026381	-0.001388	0.852506
14.085292	79.564695	4.031386	-0.001458	0.864485
16.841427	86.537845	4.036390	-0.001975	0.876636
18.551651	93.900733	4.041395	-0.002299	0.888948
19.277281	101.596072	4.046400	-0.002439	0.901342
20.246438	109.403763	4.051405	-0.002624	0.913808
21.106172	117.324378	4.056410	-0.002789	0.926249
21.922350	125.391402	4.061414	-0.002946	0.938734
22.983106	133.510700	4.066419	-0.003149	0.951197
23.682435	141.774536	4.071424	-0.003285	0.963618
24.801997	150.057520	4.076429	-0.003498	0.976014
25.754771	158.446903	4.081434	-0.003681	0.988366
26.880257	166.877601	4.086438	-0.003896	1.000665
27.634925	175.388136	4.091443	-0.004042	1.012836
28.090972	183.989855	4.096448	-0.004133	1.024916
28.571808	192.621909	4.101453	-0.004228	1.036903
29.636279	201.159194	4.106458	-0.004431	1.048761
30.568815	209.761015	4.111462	-0.004610	1.060542
31.225125	218.424547	4.116467	-0.004738	1.072211
32.488099	226.981008	4.121472	-0.004979	1.083751
33.230302	235.659091	4.126477	-0.005123	1.095210
33.669686	244.365019	4.131482	-0.005210	1.106519
34.352530	253.054524	4.136486	-0.005343	1.117745
34.916594	261.737522	4.141491	-0.005453	1.128825
35.299840	270.453158	4.146496	-0.005530	1.139800
36.000285	279.124026	4.151501	-0.005666	1.150681
36.973675	287.713355	4.156506	-0.005853	1.161418
37.631104	296.349277	4.161510	-0.005981	1.172047
38.088715	304.993788	4.166515	-0.006072	1.182549
38.552136	313.640638	4.171520	-0.006164	1.192963
39.019326	322.255823	4.176525	-0.006256	1.203249
39.456227	330.869431	4.181530	-0.006343	1.213441
40.143375	339.426841	4.186534	-0.006476	1.223531
41.181113	347.943610	4.191539	-0.006675	1.233560
41.826588	356.479486	4.196544	-0.006801	1.243454
42.764242	364.973859	4.201549	-0.006981	1.253278
43.583489	373.453310	4.206554	-0.007139	1.262987
43.981830	382.026410	4.211558	-0.007218	1.272646
44.271120	390.565053	4.216563	-0.007278	1.282173
45.277169	398.985204	4.221568	-0.007471	1.291633
46.218987	407.415235	4.226573	-0.007651	1.301022
46.272104	416.031978	4.231578	-0.007667	1.310384
47.172219	424.497337	4.236582	-0.007840	1.319670
48.207154	432.840257	4.241587	-0.008038	1.328784
48.697031	441.288165	4.246592	-0.008134	1.337850
49.270254	449.695052	4.251597	-0.008247	1.346826
49.787131	458.114234	4.256602	-0.008348	1.355746
50.476089	466.479025	4.261606	-0.008482	1.364580
50.827916	474.902204	4.266611	-0.008553	1.373360
51.430815	483.266327	4.271616	-0.008670	1.382065
52.093043	491.640638	4.276621	-0.008799	1.390737
52.689012	499.993729	4.281626	-0.008915	1.399322
53.058483	508.372860	4.286630	-0.008990	1.407843
53.526895	516.732568	4.291635	-0.009082	1.416309
54.050312	525.056280	4.296640	-0.009185	1.424698
54.521942	533.419958	4.301645	-0.009278	1.433069
54.784105	541.756027	4.306650	-0.009332	1.441329
55.572180	550.028718	4.311654	-0.009484	1.449566
55.972402	558.347705	4.316659	-0.009564	1.457738
56.585493	566.621712	4.321664	-0.009684	1.465855
57.186553	574.963781	4.326669	-0.009801	1.473991
57.685565	583.230742	4.331674	-0.009899	1.481994
58.310191	591.493348	4.336678	-0.010021	1.489969
58.783152	599.784635	4.341683	-0.010114	1.497905
59.180327	608.048002	4.346688	-0.010193	1.505761
59.990308	616.296648	4.351693	-0.010350	1.513626
60.646559	624.518933	4.356698	-0.010477	1.521401
61.479536	632.739593	4.361702	-0.010637	1.529162
62.054643	641.006897	4.366707	-0.010750	1.536888
62.420448	649.278026	4.371712	-0.010823	1.544548
62.871962	657.574958	4.376717	-0.010913	1.552205
63.238739	665.824920	4.381722	-0.010986	1.559770
63.870825	674.034909	4.386726	-0.011109	1.567301
64.692261	682.227388	4.391731	-0.011267	1.574807
65.075141	690.477154	4.396736	-0.011344	1.582265
65.447854	698.738385	4.401741	-0.011419	1.589697
66.024176	706.954283	4.406746	-0.011531	1.597083
66.527032	715.178300	4.411750	-0.011630	1.604432
66.747044	723.438244	4.416755	-0.011676	1.611738
67.266559	731.641603	4.421760	-0.011778	1.619004
67.832866	739.848263	4.426765	-0.011889	1.626247
68.077886	748.132740	4.431770	-0.011940	1.633481
68.562048	756.317912	4.436774	-0.012035	1.640629
68.953366	764.500597	4.441779	-0.012114	1.647732
69.487576	772.683001	4.446784	-0.012218	1.654823
70.005907	780.857133	4.451789	-0.012320	1.661874
70.427131	789.031246	4.456794	-0.012404	1.668883
70.802019	797.254033	4.461798	-0.012479	1.675897
71.150321	805.437838	4.466803	-0.012549	1.682845
71.678940	813.604816	4.471808	-0.012653	1.689774
71.966621	821.825664	4.476813	-0.012711	1.696688
72.248685	830.003540	4.481818	-0.012769	1.703538
72.502784	838.211909	4.486822	-0.012822	1.710381
72.902837	846.390357	4.491827	-0.012901	1.717191
73.247345	854.542048	4.496832	-0.012971	1.723945
73.446425	862.738061	4.501837	-0.013013	1.730691
73.915297	870.879360	4.506842	-0.013106	1.737400
74.476704	879.006615	4.511846	-0.013215	1.744083
74.562263	887.224451	4.516851	-0.013237	1.750753
74.697684	895.415596	4.521856	-0.013267	1.757383
75.369515	903.511759	4.526861	-0.013397	1.763979
75.652336	911.672805	4.531866	-0.013455	1.770554
75.919335	919.857559	4.536870	-0.013510	1.777121
76.518203	927.974700	4.541875	-0.013627	1.783651
77.219227	936.094701	4.546880	-0.013763	1.790172
77.967698	944.259057	4.551885	-0.013907	1.796710
78.381710	952.383841	4.556890	-0.013990	1.803152
78.633674	960.560175	4.561894	-0.014042	1.809592
79.066830	968.709295	4.566899	-0.014128	1.816009
79.478366	976.837777	4.571904	-0.014209	1.822385
80.006340	984.984868	4.576909	-0.014313	1.828767
80.185307	993.167501	4.581914	-0.014352	1.835113
80.424568	1001.317014	4.586918	-0.014401	1.841418
80.892210	1009.433385	4.591923	-0.014494	1.847704
81.226913	1017.576970	4.596928	-0.014561	1.853973
81.863867	1025.671429	4.601933	-0.014685	1.860218
82.254913	1033.791164	4.606938	-0.014763	1.866433
82.839717	1041.936846	4.611942	-0.014877	1.872670
83.270811	1050.066767	4.616947	-0.014963	1.878856
83.338787	1058.223696	4.621952	-0.014980	1.885000
84.033577	1066.320973	4.626957	-0.015115	1.891151
84.277552	1074.465403	4.631962	-0.015166	1.897266
84.595015	1082.599812	4.636966	-0.015230	1.903362
84.761609	1090.758407	4.641971	-0.015266	1.909439
85.293032	1098.855871	4.646976	-0.015370	1.915493
85.883285	1106.949155	4.651981	-0.015485	1.921531
86.084923	1115.087964	4.656986	-0.015528	1.927540
86.462320	1123.235695	4.661990	-0.015604	1.933557
86.802948	1131.346036	4.666995	-0.015672	1.939523
87.307687	1139.425039	4.672000	-0.015772	1.945466
87.762526	1147.586184	4.677005	-0.015861	1.951445
87.843293	1155.748768	4.682010	-0.015882	1.957366
88.291213	1163.815167	4.687014	-0.015970	1.963239
88.774766	1171.897321	4.692019	-0.016066	1.969110
89.329949	1179.995508	4.697024	-0.016174	1.974983
89.669708	1188.114586	4.702029	-0.016243	1.980830
89.980432	1196.226354	4.707034	-0.016306	1.986651
90.275069	1204.364588	4.712038	-0.016366	1.992472
90.644373	1212.470844	4.717043	-0.016440	1.998262
90.716067	1220.587176	4.722048	-0.016458	2.004010
91.446615	1228.649688	4.727053	-0.016599	2.009773
91.600782	1236.793887	4.732058	-0.016633	2.015517
91.734184	1244.925970	4.737062	-0.016663	2.021233
92.111890	1253.013641	4.742067	-0.016739	2.026928
92.792327	1261.091212	4.747072	-0.016871	2.032631
93.212569	1269.209642	4.752077	-0.016954	2.038319
93.351752	1277.301113	4.757082	-0.016985	2.043944
93.289465	1285.463332	4.762086	-0.016979	2.049582
93.991784	1293.507153	4.767091	-0.017115	2.055200
94.384351	1301.576167	4.772096	-0.017193	2.060789
94.933045	1309.656675	4.777101	-0.017301	2.066386
95.365372	1317.758247	4.782106	-0.017386	2.071971
95.605673	1325.876116	4.787110	-0.017436	2.077533
96.049771	1333.945381	4.792115	-0.017524	2.083066
96.792781	1341.991634	4.797120	-0.017668	2.088599
97.444168	1350.095988	4.802125	-0.017794	2.094147
97.683170	1358.209198	4.807130	-0.017844	2.099646
97.954777	1366.325459	4.812134	-0.017900	2.105136
98.370051	1374.448881	4.817139	-0.017982	2.110631
98.467193	1382.622470	4.822144	-0.018005	2.116113
99.016044	1390.662122	4.827149	-0.018113	2.121536
99.353029	1398.723958	4.832154	-0.018181	2.126939
99.768650	1406.817605	4.837158	-0.018263	2.132357
100.144240	1414.894055	4.842163	-0.018338	2.137746
100.850639	1422.915614	4.847168	-0.018475	2.143116
101.429133	1431.003888	4.852173	-0.018588	2.148505
101.595395	1439.130056	4.857178	-0.018624	2.153866
101.810362	1447.248219	4.862182	-0.018669	2.159213
102.312333	1455.298472	4.867187	-0.018768	2.164529
102.727064	1463.378458	4.872192	-0.018850	2.169843
103.154438	1471.502933	4.877197	-0.018935	2.175175
103.447038	1479.581422	4.882202	-0.018995	2.180450
103.940162	1487.650063	4.887206	-0.019092	2.185726
104.363649	1495.773333	4.892211	-0.019176	2.191017
104.680895	1503.881923	4.897216	-0.019240	2.196276
104.911338	1511.953236	4.902221	-0.019288	2.201491
105.351690	1519.979449	4.907226	-0.019375	2.206683
105.629361	1528.097838	4.912230	-0.019432	2.211907
105.928909	1536.187798	4.917235	-0.019493	2.217103
106.262218	1544.241228	4.922240	-0.019560	2.222266
106.609548	1552.319047	4.927245	-0.019630	2.227434
106.953887	1560.398328	4.932250	-0.019700	2.232591
107.328195	1568.481988	4.937254	-0.019774	2.237741
107.367604	1576.593467	4.942259	-0.019787	2.242867
107.634984	1584.648592	4.947264	-0.019842	2.247966
108.145431	1592.726888	4.952269	-0.019942	2.253089
108.369612	1600.805956	4.957274	-0.019989	2.258176
108.555952	1608.899181	4.962278	-0.020029	2.263258
108.958172	1616.961025	4.967283	-0.020109	2.268326
109.254691	1625.113781	4.972288	-0.020170	2.273431
109.807360	1633.142059	4.977293	-0.020278	2.278469
109.975620	1641.199011	4.982298	-0.020314	2.283481
110.533220	1649.225909	4.987302	-0.020423	2.288496
110.909490	1657.306415	4.992307	-0.020498	2.293518
111.246764	1665.366390	4.997312	-0.020566	2.298512
111.543591	1673.440546	5.002317	-0.020627	2.303501
111.849719	1681.512554	5.007322	-0.020689	2.308479
112.124844	1689.621004	5.012326	-0.020745	2.313466
112.504340	1697.667132	5.017331	-0.020821	2.318412
112.679558	1705.730662	5.022336	-0.020859	2.323342
112.959660	1713.816931	5.027341	-0.020916	2.328283
113.139209	1721.893335	5.032346	-0.020955	2.333200
113.461798	1729.959207	5.037350	-0.021020	2.338112
113.699926	1738.024261	5.042355	-0.021070	2.343005
114.069869	1746.090037	5.047360	-0.021144	2.347900
114.539807	1754.182998	5.052365	-0.021236	2.352809
114.824649	1762.241976	5.057370	-0.021295	2.357673
115.044891	1770.303051	5.062374	-0.021341	2.362522
115.379344	1778.355005	5.067379	-0.021408	2.367365
115.804894	1786.409066	5.072384	-0.021493	2.372207
116.292645	1794.476504	5.077389	-0.021589	2.377051
116.493756	1802.541368	5.082394	-0.021631	2.381861
116.747175	1810.616461	5.087398	-0.021684	2.386672
117.025367	1818.706031	5.092403	-0.021741	2.391483
117.123672	1826.775560	5.097408	-0.021764	2.396259
117.790539	1834.800522	5.102413	-0.021893	2.401044
118.113724	1842.836210	5.107418	-0.021959	2.405798
118.149339	1850.955795	5.112422	-0.021970	2.410570
118.580332	1859.032329	5.117427	-0.022056	2.415338
118.924688	1867.058078	5.122432	-0.022125	2.420059
119.169263	1875.133823	5.127437	-0.022176	2.424794
119.189166	1883.226804	5.132442	-0.022185	2.429511
119.689771	1891.337895	5.137446	-0.022283	2.434267
119.976770	1899.371941	5.142451	-0.022342	2.438952
120.121179	1907.399945	5.147456	-0.022374	2.443614
120.535235	1915.446312	5.152461	-0.022456	2.448298
120.963888	1923.488038	5.157466	-0.022541	2.452972
121.256960	1931.551491	5.162470	-0.022601	2.457638
121.506162	1939.616912	5.167475	-0.022652	2.462294
121.671717	1947.673571	5.172480	-0.022688	2.466930
122.028979	1955.743405	5.177485	-0.022760	2.471578
122.427832	1963.790455	5.182490	-0.022839	2.476208
122.610511	1971.851920	5.187494	-0.022879	2.480822
123.001095	1979.903436	5.192499	-0.022957	2.485436
123.100479	1987.975502	5.197504	-0.022980	2.490032
123.535601	1996.038082	5.202509	-0.023066	2.494639
123.767226	2004.090021	5.207514	-0.023115	2.499216
124.204920	2012.117561	5.212518	-0.023201	2.503786
124.631846	2020.182761	5.217523	-0.023286	2.508369
124.839430	2028.280674	5.222528	-0.023330	2.512945
125.310675	2036.318479	5.227533	-0.023423	2.517498
125.745837	2044.328441	5.232538	-0.023509	2.522025
125.970655	2052.409027	5.237542	-0.023556	2.526567
126.437717	2060.462980	5.242547	-0.023648	2.531104
126.912396	2068.485087	5.247552	-0.023742	2.535616
127.040348	2076.587311	5.252557	-0.023771	2.540140
127.248510	2084.632334	5.257562	-0.023815	2.544629
127.322012	2092.718671	5.262566	-0.023833	2.549124
127.626081	2100.795142	5.267571	-0.023895	2.553621
127.572022	2108.855755	5.272576	-0.023890	2.558077
128.129374	2116.876788	5.277581	-0.023999	2.562546
128.464897	2124.918663	5.282586	-0.024067	2.567003
128.958598	2132.974079	5.287590	-0.024164	2.571470
129.372111	2141.024056	5.292595	-0.024246	2.575921
129.807551	2149.063240	5.297600	-0.024332	2.580360
130.204010	2157.105456	5.302605	-0.024411	2.584791
130.510061	2165.165907	5.307610	-0.024474	2.589217
130.635118	2173.432809	5.312614	-0.024502	2.593736
131.104208	2181.419939	5.317619	-0.024595	2.598118
131.088825	2189.433601	5.322624	-0.024597	2.602475
131.759224	2197.416982	5.327629	-0.024727	2.606853
131.887020	2205.473909	5.332634	-0.024756	2.611228
132.428521	2213.495073	5.337638	-0.024862	2.615604
132.779839	2221.526684	5.342643	-0.024932	2.619965
132.981637	2229.544916	5.347648	-0.024975	2.624302
133.415530	2237.625634	5.352653	-0.025061	2.628681
133.751335	2245.688009	5.357658	-0.025129	2.633036
134.039607	2253.745337	5.362662	-0.025188	2.637377
134.236848	2261.796987	5.367667	-0.025229	2.641703
134.488346	2269.810886	5.372672	-0.025281	2.646005
134.739994	2277.875422	5.377677	-0.025333	2.650326
134.853817	2285.961360	5.382682	-0.025360	2.654644
135.038174	2294.003766	5.387686	-0.025399	2.658935
135.322683	2302.040000	5.392691	-0.025457	2.663223
135.308329	2310.107516	5.397696	-0.025460	2.667501
135.663885	2318.181924	5.402701	-0.025531	2.671800
135.832705	2326.239636	5.407706	-0.025568	2.676070
136.256588	2334.235003	5.412710	-0.025652	2.680318
136.463818	2342.276651	5.417715	-0.025696	2.684569
136.859780	2350.288767	5.422720	-0.025775	2.688810
137.181241	2358.373911	5.427725	-0.025840	2.693078
137.309079	2366.414985	5.432730	-0.025869	2.697303
137.721972	2374.429092	5.437734	-0.025951	2.701526
138.082452	2382.470048	5.442739	-0.026023	2.705753
138.258028	2390.525017	5.447744	-0.026061	2.709969
138.670931	2398.614584	5.452749	-0.026143	2.714211
139.100093	2406.613646	5.457754	-0.026228	2.718401
139.117918	2414.667765	5.462758	-0.026236	2.722587
139.245176	2422.766430	5.467763	-0.026265	2.726796
139.545139	2430.788391	5.472768	-0.026326	2.730970
140.126279	2438.831709	5.477773	-0.026440	2.735166
140.035322	2446.899013	5.482778	-0.026428	2.739326
140.424650	2454.901706	5.487782	-0.026505	2.743476
140.788493	2462.954956	5.492787	-0.026578	2.747644
140.804808	2471.073796	5.497792	-0.026587	2.751819
141.209812	2479.163475	5.502797	-0.026667	2.755995
141.418241	2487.150993	5.507802	-0.026711	2.760101
141.647443	2495.154198	5.512806	-0.026759	2.764211
141.958505	2503.208775	5.517811	-0.026822	2.768345
142.310906	2511.245020	5.522816	-0.026893	2.772466
142.521684	2519.309968	5.527821	-0.026937	2.776587
142.294819	2527.371095	5.532826	-0.026900	2.780674
142.519981	2535.394429	5.537830	-0.026947	2.784762
143.041925	2543.400750	5.542835	-0.027049	2.788854
143.172931	2551.472494	5.547840	-0.027079	2.792949
143.449854	2559.520119	5.552845	-0.027136	2.797035
143.855296	2567.507273	5.557850	-0.027216	2.801092
144.263800	2575.513941	5.562854	-0.027298	2.805152
144.451986	2583.592581	5.567859	-0.027338	2.809231
144.455860	2591.673200	5.572864	-0.027344	2.813293
144.999270	2599.688000	5.577869	-0.027450	2.817348
145.208025	2607.754263	5.582874	-0.027494	2.821404
145.540400	2615.760065	5.587878	-0.027561	2.825430
145.791545	2623.829886	5.592883	-0.027613	2.829478
145.916212	2631.916444	5.597888	-0.027641	2.833521
146.168642	2639.944923	5.602893	-0.027694	2.837537
146.556694	2647.952561	5.607898	-0.027771	2.841545
146.827877	2655.967381	5.612902	-0.027827	2.845543
147.057014	2664.022945	5.617907	-0.027874	2.849554
147.169606	2672.086149	5.622912	-0.027901	2.853557
147.712256	2680.104627	5.627917	-0.028007	2.857555
147.860572	2688.148729	5.632922	-0.028039	2.861539
147.891439	2696.211643	5.637926	-0.028050	2.865520
148.389401	2704.247292	5.642931	-0.028148	2.869508
148.422104	2712.313539	5.647936	-0.028160	2.873479
148.770419	2720.327050	5.652941	-0.028230	2.877437
149.119485	2728.343431	5.657946	-0.028300	2.881390
149.565856	2736.332120	5.662950	-0.028388	2.885330
149.873685	2744.397188	5.667955	-0.028450	2.889294
150.028831	2752.469378	5.672960	-0.028484	2.893247
150.361917	2760.496480	5.677965	-0.028552	2.897183
150.761922	2768.528558	5.682970	-0.028631	2.901120
151.067638	2776.546248	5.687974	-0.028693	2.905039
151.493987	2784.630398	5.692979	-0.028778	2.908991
151.612941	2792.743546	5.697984	-0.028805	2.912936
151.787731	2800.813290	5.702989	-0.028843	2.916857
152.057549	2808.802902	5.707994	-0.028898	2.920739
152.243300	2816.795057	5.712998	-0.028938	2.924613
152.652589	2824.812939	5.718003	-0.029019	2.928506
152.650756	2832.877524	5.723008	-0.029024	2.932394
153.053323	2840.926271	5.728013	-0.029104	2.936291
153.127649	2848.960570	5.733018	-0.029123	2.940159
153.369638	2856.974281	5.738022	-0.029174	2.944020
153.753527	2865.026259	5.743027	-0.029250	2.947902
153.897517	2873.078492	5.748032	-0.029282	2.951766
154.153599	2881.148849	5.753037	-0.029335	2.955640
154.191564	2889.148820	5.758042	-0.029347	2.959464
154.482418	2897.164693	5.763046	-0.029406	2.963303
154.910767	2905.190124	5.768051	-0.029491	2.967149
154.805894	2913.240040	5.773056	-0.029477	2.970975
155.166100	2921.295868	5.778061	-0.029549	2.974822
155.563049	2929.299161	5.783066	-0.029628	2.978641
155.725375	2937.326095	5.788070	-0.029664	2.982454
156.050281	2945.369847	5.793075	-0.029729	2.986278
156.221764	2953.396780	5.798080	-0.029766	2.990082
156.646871	2961.483880	5.803085	-0.029851	2.993922
156.706532	2969.538795	5.808090	-0.029867	2.997724
157.106016	2977.517665	5.813094	-0.029947	3.001502
157.465418	2985.544899	5.818099	-0.030019	3.005296
157.446142	2993.589083	5.823104	-0.030020	3.009074
157.981752	3001.635677	5.828109	-0.030125	3.012876
158.393999	3009.658329	5.833114	-0.030207	3.016656
158.631380	3017.693548	5.838118	-0.030256	3.020428
158.850695	3025.722119	5.843123	-0.030302	3.024192
159.070828	3033.741321	5.848128	-0.030348	3.027946
159.318781	3041.809911	5.853133	-0.030400	3.031720
159.646891	3049.862924	5.858138	-0.030466	3.035486
160.106101	3057.862146	5.863142	-0.030557	3.039229
160.437132	3065.907605	5.868147	-0.030623	3.042982
160.663158	3073.934970	5.873152	-0.030671	3.046717
161.019519	3081.985163	5.878157	-0.030742	3.050465
161.434342	3090.031331	5.883162	-0.030825	3.054208
161.654570	3098.053515	5.888166	-0.030871	3.057927
161.867407	3106.128971	5.893171	-0.030916	3.061665
161.927480	3114.122327	5.898176	-0.030932	3.065354
162.295145	3122.150231	5.903181	-0.031005	3.069068
162.418700	3130.277459	5.908186	-0.031034	3.072813
162.666667	3138.327217	5.913190	-0.031085	3.076523
163.020199	3146.310072	5.918195	-0.031156	3.080202
163.075696	3154.308328	5.923200	-0.031171	3.083871
163.232204	3162.343458	5.928205	-0.031206	3.087556
163.275178	3170.394271	5.933210	-0.031219	3.091239
163.472600	3178.424103	5.938214	-0.031261	3.094915
163.870721	3186.466690	5.943219	-0.031340	3.098602
164.073076	3194.460550	5.948224	-0.031383	3.102253
164.289878	3202.492008	5.953229	-0.031428	3.105918
164.411237	3210.535739	5.958234	-0.031456	3.109579
164.704856	3218.600041	5.963238	-0.031516	3.113254
164.957096	3226.626478	5.968243	-0.031568	3.116904
165.187285	3234.609474	5.973248	-0.031616	3.120530
165.379264	3242.671270	5.978253	-0.031657	3.124186
165.771556	3250.684063	5.983258	-0.031735	3.127824
166.128855	3258.724384	5.988262	-0.031807	3.131469
166.316110	3266.795880	5.993267	-0.031847	3.135115
166.452882	3274.795817	5.998272	-0.031878	3.138723
166.791324	3282.834538	6.003277	-0.031946	3.142354
167.026023	3290.853962	6.008282	-0.031995	3.145967
167.163572	3298.890146	6.013286	-0.032025	3.149578
167.688727	3306.952149	6.018291	-0.032128	3.153215
167.813561	3314.990866	6.023296	-0.032157	3.156819
168.154968	3322.983545	6.028301	-0.032225	3.160407
168.366797	3330.976381	6.033306	-0.032270	3.163986
168.540358	3339.026900	6.038310	-0.032307	3.167585
168.900149	3347.081284	6.043315	-0.032380	3.171190
169.195231	3355.128102	6.048320	-0.032440	3.174784
169.124753	3363.171615	6.053325	-0.032432	3.178358
169.249126	3371.199800	6.058330	-0.032460	3.181928
169.745289	3379.202829	6.063334	-0.032557	3.185500
170.405580	3387.214896	6.068339	-0.032686	3.189078
170.528093	3395.284126	6.073344	-0.032714	3.192654
170.836696	3403.337672	6.078349	-0.032776	3.196228
171.068342	3411.319997	6.083354	-0.032824	3.199762
171.303439	3419.349182	6.088358	-0.032873	3.203314
171.392873	3427.419631	6.093363	-0.032895	3.206874
171.588333	3435.452170	6.098368	-0.032937	3.210417
171.936229	3443.484282	6.103373	-0.033007	3.213963
172.324510	3451.490343	6.108378	-0.033084	3.217495
172.458079	3459.522206	6.113382	-0.033114	3.221024
172.701314	3467.535560	6.118387	-0.033165	3.224545
172.983760	3475.569833	6.123392	-0.033222	3.228073
173.251896	3483.657958	6.128397	-0.033277	3.231620
173.726968	3491.695064	6.133402	-0.033371	3.235150
173.938212	3499.690531	6.138406	-0.033415	3.238646
174.425084	3507.702153	6.143411	-0.033511	3.242157
174.634899	3515.690228	6.148416	-0.033555	3.245643
174.817954	3523.734010	6.153421	-0.033595	3.249148
174.842821	3531.834956	6.158426	-0.033605	3.252668
175.175891	3539.832834	6.163430	-0.033672	3.256151
175.468450	3547.844607	6.168435	-0.033731	3.259636
175.556532	3555.874451	6.173440	-0.033753	3.263116
175.670435	3563.911280	6.178445	-0.033779	3.266596
175.847135	3571.940893	6.183450	-0.033817	3.270072
176.292814	3580.007498	6.188454	-0.033905	3.273571
176.493166	3588.023362	6.193459	-0.033948	3.277034
176.395826	3596.039247	6.198464	-0.033935	3.280483
176.760214	3604.056624	6.203469	-0.034008	3.283946
176.873855	3612.100913	6.208474	-0.034034	3.287407
177.105398	3620.135123	6.213478	-0.034082	3.290865
177.723922	3628.178827	6.218483	-0.034203	3.294338
177.756086	3636.197120	6.223488	-0.034214	3.297775
177.978696	3644.227200	6.228493	-0.034260	3.301219
178.142234	3652.225751	6.233498	-0.034296	3.304645
178.359404	3660.257169	6.238502	-0.034342	3.308083
178.571008	3668.348072	6.243507	-0.034386	3.311542
178.473397	3676.396534	6.248512	-0.034373	3.314968
178.875421	3684.390730	6.253517	-0.034453	3.318387
179.039643	3692.392327	6.258522	-0.034489	3.321796
178.942682	3700.389945	6.263526	-0.034476	3.325189
179.413326	3708.438542	6.268531	-0.034569	3.328623
179.535430	3716.456255	6.273536	-0.034597	3.332026
179.668019	3724.513765	6.278541	-0.034626	3.335444
179.933458	3732.519282	6.283546	-0.034681	3.338840
180.200335	3740.532959	6.288550	-0.034736	3.342237
180.569344	3748.562322	6.293555	-0.034810	3.345641
180.592350	3756.603391	6.298560	-0.034819	3.349033
180.831758	3764.654663	6.303565	-0.034869	3.352434
181.004274	3772.711845	6.308570	-0.034906	3.355832
181.183701	3780.695717	6.313574	-0.034945	3.359196
181.584489	3788.732606	6.318579	-0.035025	3.362586
181.791254	3796.712565	6.323584	-0.035068	3.365942
182.029796	3804.734383	6.328589	-0.035118	3.369314
182.239231	3812.816067	6.333594	-0.035162	3.372706
182.674036	3820.842004	6.338598	-0.035248	3.376079
182.916936	3828.868573	6.343603	-0.035298	3.379442
183.137876	3836.893152	6.348608	-0.035345	3.382801
183.360043	3844.926462	6.353613	-0.035391	3.386159
183.680425	3852.945330	6.358618	-0.035456	3.389512
183.688046	3861.055654	6.363622	-0.035463	3.392889
183.899821	3869.127626	6.368627	-0.035507	3.396253
184.001494	3877.047023	6.373632	-0.035531	3.399547
184.264012	3885.060044	6.378637	-0.035585	3.402881
184.277692	3893.093526	6.383642	-0.035593	3.406213
184.587916	3901.065719	6.388646	-0.035656	3.409526
184.998313	3909.126567	6.393651	-0.035737	3.412876
184.939497	3917.191334	6.398656	-0.035732	3.416208
185.370923	3925.187143	6.403661	-0.035817	3.419525
185.443493	3933.199313	6.408666	-0.035836	3.422834
185.663847	3941.204089	6.413670	-0.035882	3.426141
186.043378	3949.240057	6.418675	-0.035958	3.429463
186.145213	3957.274086	6.423680	-0.035982	3.432772
186.327314	3965.347365	6.428685	-0.036021	3.436096
186.482394	3973.340993	6.433690	-0.036055	3.439383
186.775729	3981.351671	6.438694	-0.036115	3.442679
186.959857	3989.399601	6.443699	-0.036154	3.445984
186.919737	3997.392621	6.448704	-0.036152	3.449255
187.236352	4005.473629	6.453709	-0.036216	3.452571
187.713857	4013.489228	6.458714	-0.036310	3.455862
187.758369	4021.516096	6.463718	-0.036323	3.459140
187.926399	4029.563687	6.468723	-0.036360	3.462428
188.392354	4037.552279	6.473728	-0.036452	3.465698
188.623282	4045.608808	6.478733	-0.036500	3.468985
188.653736	4053.681354	6.483738	-0.036511	3.472270
188.832804	4061.692888	6.488742	-0.036549	3.475530
189.174934	4069.666047	6.493747	-0.036618	3.478778
189.172707	4077.689405	6.498752	-0.036623	3.482032
189.393908	4085.688035	6.503757	-0.036669	3.485280
189.680399	4093.741577	6.508762	-0.036728	3.488549
189.802330	4101.771682	6.513766	-0.036755	3.491800
189.957376	4109.827619	6.518771	-0.036789	3.495060
190.219323	4117.801572	6.523776	-0.036843	3.498286
190.590564	4125.807046	6.528781	-0.036918	3.501526
190.784209	4133.841641	6.533786	-0.036959	3.504770
191.123249	4141.836830	6.538790	-0.037027	3.507998
191.551013	4149.887070	6.543795	-0.037112	3.511249
191.658892	4157.915957	6.548800	-0.037137	3.514478
191.819960	4165.973101	6.553805	-0.037172	3.517717
192.028836	4173.978792	6.558810	-0.037216	3.520934
192.219010	4181.934868	6.563814	-0.037257	3.524128
192.421682	4190.002640	6.568819	-0.037300	3.527363
192.754238	4198.035245	6.573824	-0.037367	3.530586
192.996577	4206.113459	6.578829	-0.037417	3.533821
193.010472	4214.182822	6.583834	-0.037425	3.537042
193.280841	4222.172076	6.588838	-0.037480	3.540237
193.459366	4230.192831	6.593843	-0.037519	3.543438
193.529173	4238.200841	6.598848	-0.037537	3.546628
193.983485	4246.233655	6.603853	-0.037627	3.549837
194.532624	4254.325827	6.608858	-0.037734	3.553069
194.464781	4262.398390	6.613862	-0.037726	3.556271
194.692521	4270.336568	6.618867	-0.037774	3.559427
194.986793	4278.337660	6.623872	-0.037834	3.562606
195.245166	4286.344748	6.628877	-0.037887	3.565784
195.611383	4294.385899	6.633882	-0.037960	3.568976
195.570563	4302.406638	6.638886	-0.037958	3.572145
196.068989	4310.432940	6.643891	-0.038056	3.575328
196.411739	4318.412296	6.648896	-0.038125	3.578486
196.579532	4326.467876	6.653901	-0.038161	3.581666
196.864220	4334.460339	6.658906	-0.038219	3.584822
196.879394	4342.489838	6.663910	-0.038227	3.587982
197.078597	4350.560795	6.668915	-0.038270	3.591160
197.284421	4358.585242	6.673920	-0.038313	3.594318
197.549663	4366.587104	6.678925	-0.038368	3.597466
197.736522	4374.592162	6.683930	-0.038408	3.600609
197.815217	4382.594503	6.688934	-0.038427	3.603746
198.189365	4390.656202	6.693939	-0.038502	3.606912
198.135149	4398.660584	6.698944	-0.038497	3.610041
198.377788	4406.701995	6.703949	-0.038548	3.613189
198.463073	4414.764069	6.708954	-0.038569	3.616339
198.617272	4422.725050	6.713958	-0.038602	3.619448
198.862753	4430.796336	6.718963	-0.038653	3.622600
198.997617	4438.761397	6.723968	-0.038684	3.625705
199.042480	4446.819137	6.728973	-0.038697	3.628840
199.436925	4454.875555	6.733978	-0.038776	3.631982
199.693893	4462.913309	6.738982	-0.038829	3.635111
199.944281	4470.926367	6.743987	-0.038880	3.638226
200.157286	4478.931274	6.748992	-0.038925	3.641335
200.318643	4486.916852	6.753997	-0.038960	3.644433
200.474163	4494.987183	6.759002	-0.038995	3.647560
200.549011	4502.995736	6.764006	-0.039014	3.650659
200.700882	4511.060839	6.769011	-0.039047	3.653778
200.821843	4519.083234	6.774016	-0.039075	3.656878
201.062218	4527.093846	6.779021	-0.039125	3.659974
201.336285	4535.145544	6.784026	-0.039181	3.663084
201.250495	4543.140127	6.789030	-0.039170	3.666160
201.435185	4551.143451	6.794035	-0.039210	3.669243
201.539679	4559.189054	6.799040	-0.039234	3.672338
201.700057	4567.241004	6.804045	-0.039269	3.675435
201.737569	4575.235595	6.809050	-0.039281	3.678503
202.009128	4583.244093	6.814054	-0.039337	3.681581
202.097197	4591.210466	6.819059	-0.039358	3.684635
202.231874	4599.270165	6.824064	-0.039389	3.687723
202.646333	4607.278183	6.829069	-0.039471	3.690796
202.788435	4615.334714	6.834074	-0.039503	3.693878
202.789949	4623.359829	6.839078	-0.039508	3.696942
203.167754	4631.375973	6.844083	-0.039584	3.700009
203.412553	4639.369114	6.849088	-0.039634	3.703062
203.521235	4647.381928	6.854093	-0.039660	3.706116
203.752610	4655.430380	6.859098	-0.039708	3.709185
203.999029	4663.492025	6.864102	-0.039759	3.712256
204.246888	4671.587502	6.869107	-0.039810	3.715337
204.414321	4679.521368	6.874112	-0.039847	3.718353
204.694346	4687.528651	6.879117	-0.039904	3.721396
204.801123	4695.501772	6.884122	-0.039929	3.724420
204.799101	4703.530429	6.889126	-0.039934	3.727460
205.333917	4711.545569	6.894131	-0.040038	3.730505
205.366198	4719.605118	6.899136	-0.040049	3.733553
205.655567	4727.640981	6.904141	-0.040108	3.736595
205.783845	4735.631600	6.909146	-0.040138	3.739614
205.834467	4743.671713	6.914150	-0.040152	3.742647
206.039869	4751.697087	6.919155	-0.040195	3.745675
206.229235	4759.726736	6.924160	-0.040236	3.748703
206.550766	4767.758069	6.929165	-0.040301	3.751731
206.844520	4775.798594	6.934170	-0.040361	3.754760
206.899018	4783.783188	6.939174	-0.040376	3.757760
206.942331	4791.830647	6.944179	-0.040389	3.760781
207.122046	4799.822084	6.949184	-0.040428	3.763782
207.313208	4807.847627	6.954189	-0.040469	3.766793
207.572405	4815.903898	6.959194	-0.040522	3.769815
207.853067	4823.908670	6.964198	-0.040579	3.772815
208.065987	4831.971683	6.969203	-0.040624	3.775833
208.121324	4839.982192	6.974208	-0.040640	3.778826
208.401054	4847.968826	6.979213	-0.040697	3.781813
208.642066	4855.980980	6.984218	-0.040747	3.784805
208.650573	4864.006795	6.989222	-0.040754	3.787796
209.058976	4872.079713	6.994227	-0.040835	3.790810
209.494437	4880.108934	6.999232	-0.040921	3.793806
209.862315	4888.113411	7.004237	-0.040995	3.796789
209.902460	4896.085675	7.009242	-0.041007	3.799751
210.062458	4904.096686	7.014246	-0.041042	3.802727
210.348554	4912.120972	7.019251	-0.041101	3.805708
210.390361	4920.142362	7.024256	-0.041114	3.808681
210.503946	4928.206357	7.029261	-0.041140	3.811669
210.493302	4936.220627	7.034266	-0.041143	3.814633
210.722508	4944.226404	7.039270	-0.041191	3.817597
210.994854	4952.223335	7.044275	-0.041247	3.820557
211.236966	4960.239331	7.049280	-0.041297	3.823520
211.510481	4968.280187	7.054285	-0.041353	3.826491
211.516607	4976.301155	7.059290	-0.041359	3.829447
211.777786	4984.329929	7.064294	-0.041413	3.832408
212.121774	4992.385805	7.069299	-0.041482	3.835379
211.987836	5000.360404	7.074304	-0.041462	3.838308
212.293744	5008.368130	7.079309	-0.041524	3.841256
212.410422	5016.397874	7.084314	-0.041551	3.844205
212.288532	5024.407167	7.089318	-0.041534	3.847140
212.748324	5032.457426	7.094323	-0.041625	3.850100
212.778571	5040.465455	7.099328	-0.041635	3.853033
212.754032	5048.490321	7.104333	-0.041636	3.855969
212.919426	5056.550113	7.109338	-0.041672	3.858919
212.978337	5064.564732	7.114342	-0.041688	3.861849
213.345959	5072.567702	7.119347	-0.041762	3.864778
213.601617	5080.601856	7.124352	-0.041814	3.867714
213.751033	5088.630873	7.129357	-0.041847	3.870643
214.083299	5096.866215	7.134362	-0.041914	3.873650
214.086006	5104.857307	7.139366	-0.041920	3.876558
214.375675	5112.751375	7.144371	-0.041979	3.879435
214.501603	5120.758182	7.149376	-0.042008	3.882347
214.782024	5128.708627	7.154381	-0.042065	3.885239
215.037202	5136.760283	7.159386	-0.042118	3.888166
215.139662	5144.750421	7.164390	-0.042142	3.891065
215.391620	5152.846421	7.169395	-0.042194	3.894003
215.482550	5160.844981	7.174400	-0.042216	3.896901
215.614662	5168.799036	7.179405	-0.042246	3.899781
216.089083	5176.850007	7.184410	-0.042339	3.902700
216.187136	5184.856774	7.189414	-0.042363	3.905594
216.501776	5192.869546	7.194419	-0.042426	3.908492
216.497755	5200.911797	7.199424	-0.042431	3.911393
216.595309	5208.945263	7.204429	-0.042454	3.914290
216.835064	5216.986978	7.209434	-0.042504	3.917191
217.003098	5224.932552	7.214438	-0.042540	3.920053
217.384943	5232.966058	7.219443	-0.042616	3.922949
217.650923	5240.951574	7.224448	-0.042671	3.925824
217.788963	5248.997361	7.229453	-0.042702	3.928715
218.194404	5257.040914	7.234458	-0.042783	3.931609
218.124924	5265.038585	7.239462	-0.042775	3.934475
218.304649	5273.113311	7.244467	-0.042813	3.937371
218.431889	5281.112060	7.249472	-0.042842	3.940237
218.741216	5289.097201	7.254477	-0.042905	3.943100
218.972467	5297.106110	7.259482	-0.042953	3.945967
219.115088	5305.104323	7.264486	-0.042985	3.948827
219.369266	5313.183432	7.269491	-0.043037	3.951715
219.455421	5321.225100	7.274496	-0.043059	3.954585
219.547844	5329.272350	7.279501	-0.043081	3.957455
219.998868	5337.226607	7.284506	-0.043170	3.960296
220.362729	5345.158505	7.289510	-0.043243	3.963126
220.488640	5353.207745	7.294515	-0.043271	3.965991
220.451257	5361.268030	7.299520	-0.043270	3.968855
220.773924	5369.311725	7.304525	-0.043335	3.971717
220.917272	5377.360181	7.309530	-0.043367	3.974576
221.111283	5385.383930	7.314534	-0.043408	3.977425
221.277548	5393.385742	7.319539	-0.043444	3.980263
221.458633	5401.390005	7.324544	-0.043483	3.983101
221.579487	5409.390510	7.329549	-0.043511	3.985934
221.784105	5417.456466	7.334554	-0.043554	3.988790
221.719489	5425.505385	7.339558	-0.043547	3.991633
221.855568	5433.516295	7.344563	-0.043577	3.994464
222.072074	5441.557590	7.349568	-0.043623	3.997305
222.127988	5449.511948	7.354573	-0.043638	4.000111
222.463626	5457.546958	7.359578	-0.043706	4.002948
222.555750	5465.556258	7.364582	-0.043728	4.005769
222.846523	5473.591595	7.369587	-0.043788	4.008601
222.722748	5481.660215	7.374592	-0.043770	4.011436
222.773312	5489.679606	7.379597	-0.043784	4.014255
223.067872	5497.740957	7.384602	-0.043844	4.017090
223.179984	5505.675573	7.389606	-0.043870	4.019876
223.379833	5513.708079	7.394611	-0.043913	4.022695
223.388413	5521.731527	7.399616	-0.043919	4.025507
223.709148	5529.746961	7.404621	-0.043984	4.028318
224.000748	5537.785470	7.409626	-0.044044	4.031135
224.000066	5545.872754	7.414630	-0.044049	4.033962
224.297655	5553.914430	7.419635	-0.044109	4.036777
224.494701	5561.819466	7.424640	-0.044151	4.039540
224.467670	5569.845194	7.429645	-0.044151	4.042339
224.694171	5577.845103	7.434650	-0.044199	4.045132
224.776935	5585.841486	7.439654	-0.044219	4.047919
225.049865	5593.899995	7.444659	-0.044275	4.050729
225.088960	5601.895035	7.449664	-0.044287	4.053512
225.268289	5609.922076	7.454669	-0.044326	4.056305
225.357010	5617.937822	7.459674	-0.044348	4.059091
225.328670	5625.940574	7.464678	-0.044348	4.061870
225.728858	5633.913165	7.469683	-0.044427	4.064642
226.085155	5641.977837	7.474688	-0.044499	4.067443
226.239986	5649.968106	7.479693	-0.044533	4.070214
226.584736	5658.060814	7.484698	-0.044602	4.073021
226.617305	5666.041887	7.489702	-0.044613	4.075783
226.687383	5674.054886	7.494707	-0.044631	4.078555
226.792028	5682.071990	7.499712	-0.044656	4.081326
227.040215	5690.036428	7.504717	-0.044707	4.084080
227.370831	5698.065535	7.509722	-0.044774	4.086855
227.350008	5706.084202	7.514726	-0.044775	4.089620
227.272756	5714.176665	7.519731	-0.044766	4.092408
227.502210	5722.186478	7.524736	-0.044814	4.095169
227.532158	5730.197745	7.529741	-0.044825	4.097926
227.922276	5738.217774	7.534746	-0.044902	4.100690
228.079495	5746.176904	7.539750	-0.044937	4.103427
228.229896	5754.249895	7.544755	-0.044970	4.106202
228.141504	5762.291999	7.549760	-0.044959	4.108960
228.559398	5770.310305	7.554765	-0.045042	4.111716
228.609376	5778.369889	7.559770	-0.045056	4.114479
228.775555	5786.351239	7.564774	-0.045092	4.117215
228.861984	5794.340945	7.569779	-0.045113	4.119951
229.136122	5802.353699	7.574784	-0.045170	4.122695
229.187270	5810.340846	7.579789	-0.045184	4.125426
229.341473	5818.390790	7.584794	-0.045218	4.128177
229.480575	5826.376282	7.589798	-0.045249	4.130905
229.711476	5834.466320	7.594803	-0.045297	4.133668
229.755856	5842.523715	7.599808	-0.045311	4.136415
230.071767	5850.495160	7.604813	-0.045375	4.139135
230.390553	5858.543434	7.609818	-0.045439	4.141879
230.344242	5866.493568	7.614822	-0.045436	4.144583
230.594452	5874.576192	7.619827	-0.045487	4.147334
230.796110	5882.555702	7.624832	-0.045530	4.150048
230.989115	5890.612567	7.629837	-0.045571	4.152786
231.033258	5898.669881	7.634842	-0.045585	4.155520
231.215977	5906.626437	7.639846	-0.045624	4.158220
231.572341	5914.649559	7.644851	-0.045695	4.160943
231.808950	5922.650825	7.649856	-0.045744	4.163656
232.039827	5930.680678	7.654861	-0.045793	4.166376
232.276127	5938.687995	7.659866	-0.045842	4.169087
232.136065	5946.731737	7.664870	-0.045821	4.171804
232.425904	5954.757085	7.669875	-0.045880	4.174518
232.736769	5962.755628	7.674880	-0.045943	4.177221
232.791394	5970.722569	7.679885	-0.045958	4.179909
232.847455	5978.795602	7.684890	-0.045974	4.182631
233.260294	5986.731589	7.689894	-0.046056	4.185309
233.556503	5994.830599	7.694899	-0.046116	4.188039
233.535277	6002.814358	7.699904	-0.046117	4.190725
233.588500	6010.919747	7.704909	-0.046132	4.193451
233.929083	6019.005502	7.709914	-0.046201	4.196171
233.925349	6026.894551	7.714918	-0.046205	4.198820
234.173476	6034.936093	7.719923	-0.046257	4.201522
234.421094	6042.883291	7.724928	-0.046308	4.204189
234.473634	6050.884562	7.729933	-0.046323	4.206871
234.501979	6058.934605	7.734938	-0.046333	4.209568
234.451752	6066.963312	7.739942	-0.046329	4.212255
234.798323	6075.007461	7.744947	-0.046399	4.214949
234.921118	6083.026304	7.749952	-0.046427	4.217631
234.947716	6090.969065	7.754957	-0.046437	4.220285
235.243183	6099.025743	7.759962	-0.046497	4.222977
235.328774	6107.007802	7.764966	-0.046518	4.225641
235.558256	6115.054391	7.769971	-0.046566	4.228327
235.653289	6123.078265	7.774976	-0.046589	4.231001
235.801226	6131.159181	7.779981	-0.046621	4.233694
235.895064	6139.187750	7.784986	-0.046644	4.236366
236.173533	6147.123177	7.789990	-0.046701	4.239008
236.444574	6155.182276	7.794995	-0.046757	4.241689
236.617473	6163.145006	7.800000	-0.046794	4.244336
236.646906	6171.213717	7.805005	-0.046805	4.247015
236.922552	6179.192179	7.810010	-0.046861	4.249664
237.011806	6187.228005	7.815014	-0.046883	4.252329
237.043236	6195.272391	7.820019	-0.046894	4.254994
237.320570	6203.307577	7.825024	-0.046951	4.257657
237.392086	6211.298759	7.830029	-0.046969	4.260302
237.674524	6219.327982	7.835034	-0.047027	4.262960
237.671462	6227.279255	7.840038	-0.047031	4.265588
237.866018	6235.349330	7.845043	-0.047073	4.268255
237.860725	6243.391959	7.850048	-0.047077	4.270910
238.063489	6251.452144	7.855053	-0.047120	4.273570
238.379699	6259.480393	7.860058	-0.047184	4.276220
238.322953	6267.418148	7.865062	-0.047178	4.278834
238.374146	6275.489822	7.870067	-0.047193	4.281492
238.646388	6283.392943	7.875072	-0.047249	4.284095
238.922760	6291.470873	7.880077	-0.047305	4.286754
239.004703	6299.484676	7.885082	-0.047326	4.289388
238.867881	6307.545953	7.890086	-0.047306	4.292035
239.271968	6315.556988	7.895091	-0.047386	4.294668
239.566169	6323.578648	7.900096	-0.047446	4.297301
239.628544	6331.531900	7.905101	-0.047463	4.299909
239.781774	6339.605074	7.910106	-0.047496	4.302555
239.787580	6347.582837	7.915110	-0.047502	4.305167
239.808050	6355.622370	7.920115	-0.047511	4.307798
240.066663	6363.654569	7.925120	-0.047565	4.310427
240.284051	6371.690829	7.930125	-0.047610	4.313055
240.393616	6379.702063	7.935130	-0.047636	4.315673
240.460185	6387.684752	7.940134	-0.047653	4.318279
240.725282	6395.683117	7.945139	-0.047708	4.320890
240.737860	6403.709348	7.950144	-0.047715	4.323507
240.637626	6411.706544	7.955149	-0.047702	4.326112
241.120593	6419.756075	7.960154	-0.047797	4.328737
241.110954	6427.767731	7.965158	-0.047800	4.331344
241.189719	6435.798625	7.970163	-0.047820	4.333956
241.345397	6443.846201	7.975168	-0.047854	4.336573
241.597603	6451.822628	7.980173	-0.047906	4.339166
241.836241	6459.858090	7.985178	-0.047956	4.341776
241.899761	6467.813598	7.990182	-0.047973	4.344358
242.184229	6475.876200	7.995187	-0.048031	4.346974
242.474860	6483.854995	8.000192	-0.048090	4.349562
242.415153	6491.882426	8.005197	-0.048084	4.352161
242.690171	6500.047810	8.010202	-0.048141	4.354806
242.821885	6508.048315	8.015206	-0.048170	4.357394
242.868926	6515.936488	8.020211	-0.048184	4.359945
242.946328	6523.990133	8.025216	-0.048204	4.362547
243.208400	6531.939631	8.030221	-0.048258	4.365116
243.327204	6540.028281	8.035226	-0.048285	4.367727
243.518489	6547.962613	8.040230	-0.048326	4.370287
243.760727	6556.032497	8.045235	-0.048376	4.372889
243.942576	6564.080300	8.050240	-0.048415	4.375483
243.940590	6572.076190	8.055245	-0.048420	4.378057
244.167874	6580.069713	8.060250	-0.048467	4.380630
244.289488	6588.051481	8.065254	-0.048495	4.383197
244.292816	6596.093537	8.070259	-0.048501	4.385782
244.387902	6604.139704	8.075264	-0.048523	4.388366
244.653008	6612.142946	8.080269	-0.048578	4.390937
244.852749	6620.198845	8.085274	-0.048620	4.393522
244.747022	6628.208274	8.090278	-0.048606	4.396089
244.925179	6636.158122	8.095283	-0.048644	4.398637
245.105690	6644.214044	8.100288	-0.048683	4.401218
245.111382	6652.209338	8.105293	-0.048689	4.403777
245.323630	6660.254758	8.110298	-0.048734	4.406351
245.700934	6668.245665	8.115302	-0.048809	4.408908
245.633232	6676.311957	8.120307	-0.048802	4.411484
245.790899	6684.367681	8.125312	-0.048836	4.414057
246.078210	6692.388984	8.130317	-0.048895	4.416618
246.355413	6700.341774	8.135322	-0.048952	4.419156
246.369088	6708.376708	8.140326	-0.048959	4.421716
246.557647	6716.363714	8.145331	-0.048999	4.424262
246.861679	6724.428259	8.150336	-0.049061	4.426830
246.883020	6732.421224	8.155341	-0.049070	4.429374
246.999474	6740.485206	8.160346	-0.049097	4.431938
247.001140	6748.477898	8.165350	-0.049103	4.434478
247.090283	6756.560491	8.170355	-0.049124	4.437046
247.088665	6764.488691	8.175360	-0.049129	4.439562
247.278095	6772.511347	8.180365	-0.049170	4.442108
247.475135	6780.485399	8.185370	-0.049211	4.444638
247.660491	6788.534203	8.190374	-0.049251	4.447189
247.786096	6796.536221	8.195379	-0.049280	4.449724
248.107836	6804.616333	8.200384	-0.049345	4.452282
248.060812	6812.575539	8.205389	-0.049341	4.454800
248.232710	6820.652104	8.210394	-0.049378	4.457354
248.411256	6828.625568	8.215398	-0.049417	4.459874
248.643787	6836.669231	8.220403	-0.049465	4.462415
248.724680	6844.668897	8.225408	-0.049485	4.464940
248.977002	6852.664219	8.230413	-0.049537	4.467463
249.232574	6860.681962	8.235418	-0.049590	4.469992
249.133334	6868.746973	8.240422	-0.049577	4.472532
249.265347	6876.721768	8.245427	-0.049606	4.475044
249.487196	6884.763641	8.250432	-0.049653	4.477576
249.572858	6892.725223	8.255437	-0.049674	4.480080
249.615498	6900.778177	8.260442	-0.049687	4.482612
249.564504	6908.741240	8.265446	-0.049683	4.485113
249.810719	6916.790298	8.270451	-0.049734	4.487642
249.894853	6924.791855	8.275456	-0.049754	4.490153
250.001448	6932.820616	8.280461	-0.049779	4.492672
250.309281	6940.847055	8.285466	-0.049842	4.495188
250.288927	6948.881150	8.290470	-0.049843	4.497705
250.424434	6956.868469	8.295475	-0.049874	4.500207
250.604192	6964.914787	8.300480	-0.049912	4.502725
250.683622	6972.875694	8.305485	-0.049932	4.505215
250.953214	6980.907372	8.310490	-0.049988	4.507727
251.133586	6988.905394	8.315494	-0.050026	4.510226
251.418275	6996.995105	8.320499	-0.050084	4.512753
251.560630	7005.046557	8.325504	-0.050116	4.515265
251.485407	7013.001094	8.330509	-0.050107	4.517746
251.769153	7020.963310	8.335514	-0.050165	4.520229
251.766194	7028.990246	8.340518	-0.050170	4.522730
251.877312	7036.976694	8.345523	-0.050196	4.525217
251.973852	7045.011841	8.350528	-0.050219	4.527717
252.155248	7053.031831	8.355533	-0.050258	4.530212
252.427378	7061.124045	8.360538	-0.050313	4.532728
252.592186	7069.123038	8.365542	-0.050349	4.535213
252.823692	7077.077809	8.370547	-0.050397	4.537684
252.998425	7085.137978	8.375552	-0.050435	4.540186
252.960386	7093.090112	8.380557	-0.050433	4.542652
253.181779	7101.134785	8.385562	-0.050480	4.545146
253.297186	7109.146234	8.390566	-0.050506	4.547628
253.507660	7117.144480	8.395571	-0.050550	4.550105
253.644361	7125.254500	8.400576	-0.050581	4.552616
253.769860	7133.279254	8.405581	-0.050610	4.555098
253.864939	7141.319692	8.410586	-0.050633	4.557584
253.973569	7149.186617	8.415590	-0.050658	4.560014
254.068571	7157.264146	8.420595	-0.050681	4.562509
254.254463	7165.249655	8.425600	-0.050720	4.564974
254.371101	7173.298540	8.430605	-0.050747	4.567457
254.741541	7181.282070	8.435610	-0.050821	4.569918
254.738487	7189.336184	8.440614	-0.050826	4.572400
254.791205	7197.338730	8.445619	-0.050841	4.574864
254.845286	7205.386200	8.450624	-0.050856	4.577341
255.189018	7213.350958	8.455629	-0.050925	4.579792
255.367651	7221.456658	8.460634	-0.050964	4.582284
255.303399	7229.368248	8.465638	-0.050957	4.584715
255.391488	7237.474839	8.470643	-0.050978	4.587205
255.629901	7245.469595	8.475648	-0.051028	4.589659
255.684535	7253.463977	8.480653	-0.051043	4.592112
255.940261	7261.505108	8.485658	-0.051096	4.594578
256.133493	7269.541586	8.490662	-0.051137	4.597041
256.204860	7277.530610	8.495667	-0.051156	4.599488
256.499290	7285.599178	8.500672	-0.051216	4.601958
256.610232	7293.493746	8.505677	-0.051241	4.604373
256.821869	7301.586470	8.510682	-0.051286	4.606848
256.733473	7309.539709	8.515686	-0.051274	4.609279
256.837627	7317.584984	8.520691	-0.051299	4.611737
257.026040	7325.650959	8.525696	-0.051339	4.614199
257.224776	7333.649687	8.530701	-0.051381	4.616640
257.363976	7341.644523	8.535706	-0.051412	4.619078
257.344970	7349.630247	8.540710	-0.051414	4.621513
257.513767	7357.657213	8.545715	-0.051451	4.623958
257.805111	7365.686561	8.550720	-0.051510	4.626403
257.901509	7373.687229	8.555725	-0.051533	4.628838
258.002803	7381.748627	8.560730	-0.051557	4.631290
257.942754	7389.761718	8.565735	-0.051551	4.633726
258.274323	7397.758083	8.570739	-0.051618	4.636155
258.576757	7405.762838	8.575744	-0.051679	4.638586
258.656204	7413.778658	8.580749	-0.051699	4.641019
258.894506	7421.805258	8.585754	-0.051749	4.643454
258.931115	7429.799629	8.590759	-0.051761	4.645878
259.135537	7437.783184	8.595763	-0.051804	4.648297
259.141894	7445.835375	8.600768	-0.051810	4.650736
259.310165	7453.877853	8.605773	-0.051847	4.653171
259.407114	7461.930579	8.610778	-0.051870	4.655607
259.685421	7469.897317	8.615783	-0.051927	4.658016
259.953886	7477.876524	8.620787	-0.051982	4.660427
260.034346	7485.939888	8.625792	-0.052002	4.662863
259.933863	7493.873360	8.630797	-0.051989	4.665259
260.148258	7501.941554	8.635802	-0.052034	4.667693
260.272432	7509.962921	8.640807	-0.052062	4.670112
260.733724	7518.044957	8.645811	-0.052153	4.672548
260.801088	7526.092196	8.650816	-0.052171	4.674973
261.016826	7534.075946	8.655821	-0.052216	4.677377
261.138859	7542.028133	8.660826	-0.052244	4.679770
261.061455	7550.051884	8.665831	-0.052235	4.682184
261.233129	7557.967935	8.670835	-0.052272	4.684564
261.468948	7566.090045	8.675840	-0.052321	4.687004
261.673710	7574.006289	8.680845	-0.052364	4.689382
261.965756	7582.082163	8.685850	-0.052423	4.691806
262.230254	7590.094512	8.690855	-0.052478	4.694209
262.231364	7598.148921	8.695859	-0.052483	4.696625
262.346444	7606.111364	8.700864	-0.052510	4.699011
262.607158	7614.164390	8.705869	-0.052563	4.701423
262.804893	7622.172195	8.710874	-0.052605	4.703821
262.666814	7630.180665	8.715879	-0.052585	4.706218
262.886645	7638.147841	8.720883	-0.052631	4.708600
263.132474	7646.277067	8.725888	-0.052682	4.711030
263.237814	7654.245408	8.730893	-0.052707	4.713411
263.416982	7662.295798	8.735898	-0.052745	4.715815
263.522911	7670.282812	8.740903	-0.052770	4.718199
263.667283	7678.244935	8.745907	-0.052802	4.720574
263.756198	7686.310132	8.750912	-0.052824	4.722979
263.960838	7694.268403	8.755917	-0.052867	4.725351
264.103674	7702.354939	8.760922	-0.052899	4.727759
264.182216	7710.322357	8.765927	-0.052918	4.730131
264.506302	7718.428352	8.770931	-0.052984	4.732543
264.691769	7726.415490	8.775936	-0.053024	4.734918
264.635182	7734.427441	8.780941	-0.053018	4.737300
264.879385	7742.422262	8.785946	-0.053069	4.739675
265.255006	7750.475114	8.790951	-0.053144	4.742066
265.552815	7758.438794	8.795955	-0.053204	4.744429
265.606526	7766.479751	8.800960	-0.053220	4.746814
265.787105	7774.486140	8.805965	-0.053258	4.749188
266.006038	7782.500194	8.810970	-0.053304	4.751562
265.998839	7790.548490	8.815975	-0.053308	4.753947
266.107598	7798.557859	8.820979	-0.053333	4.756318
266.417476	7806.531402	8.825984	-0.053396	4.758676
266.469389	7814.532375	8.830989	-0.053411	4.761043
266.518919	7822.570071	8.835994	-0.053425	4.763419
266.764321	7830.544448	8.840999	-0.053476	4.765775
266.787913	7838.560302	8.846003	-0.053486	4.768142
266.858059	7846.613535	8.851008	-0.053504	4.770519
267.087929	7854.624176	8.856013	-0.053552	4.772882
267.333561	7862.682501	8.861018	-0.053603	4.775257
267.567380	7870.709825	8.866023	-0.053652	4.777623
267.615157	7878.634861	8.871027	-0.053665	4.779957
267.725326	7886.705688	8.876032	-0.053691	4.782333
267.703076	7894.637642	8.881037	-0.053692	4.784668
267.840765	7902.712638	8.886042	-0.053723	4.787043
267.972325	7910.711964	8.891047	-0.053753	4.789394
268.059180	7918.707199	8.896051	-0.053774	4.791744
268.183709	7926.791996	8.901056	-0.053802	4.794118
268.314546	7934.766076	8.906061	-0.053832	4.796459
268.738514	7942.785727	8.911066	-0.053916	4.798810
268.811922	7950.790342	8.916071	-0.053935	4.801158
268.866743	7958.783712	8.921075	-0.053950	4.803501
269.119528	7966.834174	8.926080	-0.054002	4.805858
269.092511	7974.810727	8.931085	-0.054002	4.808195
269.476144	7982.849957	8.936090	-0.054079	4.810546
269.551121	7990.286346	8.941095	-0.054098	4.812721
269.755036	7994.889244	8.946099	-0.054138	4.814067
269.917398	7997.441493	8.951104	-0.054170	4.814812
269.927295	7998.748645	8.956109	-0.054173	4.815194
270.124993	7999.221720	8.961114	-0.054210	4.815332
270.094508	8000.299817	8.966119	-0.054205	4.815647
269.925280	8000.239378	8.971123	-0.054173	4.815630
270.163947	8000.294527	8.976128	-0.054218	4.815645
270.248203	8000.267060	8.981133	-0.054233	4.815637
270.203151	8000.230007	8.986138	-0.054225	4.815626
270.471930	8000.207688	8.991143	-0.054275	4.815618
270.502150	8000.169727	8.996147	-0.054280	4.815607
270.698891	8000.272252	9.001152	-0.054317	4.815636
270.723782	8000.282262	9.006157	-0.054321	4.815639
270.678835	8000.312492	9.011162	-0.054313	4.815648
270.515396	8000.289525	9.016167	-0.054282	4.815642
270.578241	8000.226466	9.021171	-0.054294	4.815623
270.786544	8000.312092	9.026176	-0.054333	4.815647
270.768111	8000.244502	9.031181	-0.054329	4.815628
270.703678	8000.243442	9.036186	-0.054317	4.815628
270.724466	8000.190376	9.041191	-0.054321	4.815612
270.839784	8000.150600	9.046195	-0.054342	4.815600
270.838515	8000.201835	9.051200	-0.054342	4.815615
270.857234	8000.141259	9.056205	-0.054345	4.815597
271.015114	8000.208975	9.061210	-0.054375	4.815616
271.085074	8000.283800	9.066215	-0.054388	4.815638
271.110623	8000.270326	9.071219	-0.054392	4.815634
271.248980	8000.317433	9.076224	-0.054418	4.815647
271.176335	8000.244684	9.081229	-0.054404	4.815626
271.176316	8000.245745	9.086234	-0.054404	4.815626
270.918827	8000.259689	9.091239	-0.054356	4.815631
271.005309	8000.217306	9.096243	-0.054372	4.815619
271.053605	8000.276826	9.101248	-0.054381	4.815636
270.994474	8000.220318	9.106253	-0.054370	4.815620
271.153889	8000.276313	9.111258	-0.054400	4.815635
271.362860	8000.238066	9.116263	-0.054438	4.815623
271.118290	8000.228725	9.121267	-0.054393	4.815621
271.143622	8000.344473	9.126272	-0.054397	4.815655
271.113053	8000.353579	9.131277	-0.054392	4.815658
271.328567	8000.340003	9.136282	-0.054432	4.815653
271.117000	8000.287413	9.141287	-0.054392	4.815639
271.243429	8000.269179	9.146291	-0.054416	4.815633
271.409929	8000.359465	9.151296	-0.054447	4.815658
271.283277	8000.267678	9.156301	-0.054423	4.815632
271.519692	8000.255512	9.161306	-0.054467	4.815627
271.571408	8000.333244	9.166311	-0.054476	4.815650
271.436471	8000.288314	9.171315	-0.054451	4.815637
271.547534	8000.333908	9.176320	-0.054472	4.815650
271.482951	8000.240998	9.181325	-0.054460	4.815623
271.572180	8000.214680	9.186330	-0.054476	4.815615
271.474937	8000.268620	9.191335	-0.054458	4.815631
271.475749	8000.271830	9.196339	-0.054458	4.815632
271.541338	8000.300661	9.201344	-0.054470	4.815641
271.379123	8000.264897	9.206349	-0.054440	4.815631
271.608374	8000.240866	9.211354	-0.054483	4.815623
271.622606	8000.294490	9.216359	-0.054485	4.815638
271.698344	8000.230572	9.221363	-0.054499	4.815619
271.675302	8000.260092	9.226368	-0.054495	4.815628
271.816532	8000.257051	9.231373	-0.054521	4.815626
271.881601	8000.322187	9.236378	-0.054533	4.815645
271.687059	8000.338226	9.241383	-0.054497	4.815651
271.718670	8000.246887	9.246387	-0.054502	4.815624
271.878837	8000.297555	9.251392	-0.054532	4.815638
271.726962	8000.234192	9.256397	-0.054504	4.815620
271.704444	8000.286148	9.261402	-0.054500	4.815636
271.784460	8000.317351	9.266407	-0.054514	4.815644
271.884310	8000.273051	9.271411	-0.054533	4.815631
271.947830	8000.331753	9.276416	-0.054545	4.815648
271.863906	8000.315423	9.281421	-0.054529	4.815643
271.906602	8000.283005	9.286426	-0.054537	4.815634
271.960313	8000.314847	9.291431	-0.054547	4.815643
272.161463	8000.288221	9.296435	-0.054584	4.815634
272.289969	8000.335169	9.301440	-0.054608	4.815647
272.238926	8000.310831	9.306445	-0.054598	4.815640
272.309058	8000.306630	9.311450	-0.054611	4.815639
272.189360	8000.301463	9.316455	-0.054589	4.815638
272.033432	8000.258324	9.321459	-0.054560	4.815626
272.027504	8000.323368	9.326464	-0.054559	4.815645
272.074145	8000.286742	9.331469	-0.054567	4.815634
272.232879	8000.327776	9.336474	-0.054597	4.815645
272.144385	8000.337003	9.341479	-0.054580	4.815648
272.179226	8000.273484	9.346483	-0.054587	4.815630
272.245912	8000.348259	9.351488	-0.054599	4.815651
272.075781	8000.276052	9.356493	-0.054567	4.815631
272.008567	8000.298442	9.361498	-0.054555	4.815638
272.251164	8000.301330	9.366503	-0.054600	4.815637
272.310881	8000.248898	9.371507	-0.054611	4.815622
272.299762	8000.277545	9.376512	-0.054608	4.815630
272.186999	8000.259675	9.381517	-0.054587	4.815626
272.286202	8000.273036	9.386522	-0.054606	4.815629
272.205437	8000.312294	9.391527	-0.054591	4.815641
272.271527	8000.257830	9.396531	-0.054603	4.815625
272.563880	8000.311727	9.401536	-0.054657	4.815639
272.158850	8000.248498	9.406541	-0.054582	4.815622
272.109461	8000.282928	9.411546	-0.054572	4.815633
272.272498	8000.314420	9.416551	-0.054603	4.815641
272.290607	8000.241016	9.421555	-0.054606	4.815620
272.341885	8000.309131	9.426560	-0.054615	4.815639
272.166073	8000.235763	9.431565	-0.054583	4.815619
272.183217	8000.265939	9.436570	-0.054586	4.815627
272.226370	8000.349942	9.441575	-0.054594	4.815652
272.170656	8000.215523	9.446579	-0.054583	4.815613
272.412217	8000.274998	9.451584	-0.054628	4.815629
272.285790	8000.193893	9.456589	-0.054604	4.815606
272.351667	8000.252634	9.461594	-0.054617	4.815623
272.172679	8000.218730	9.466599	-0.054583	4.815614
272.446049	8000.194352	9.471603	-0.054634	4.815605
272.531335	8000.247003	9.476608	-0.054650	4.815620
272.460397	8000.195640	9.481613	-0.054637	4.815606
272.576819	8000.192194	9.486618	-0.054658	4.815604
272.528889	8000.251212	9.491623	-0.054649	4.815621
272.509421	8000.180398	9.496627	-0.054645	4.815601
272.640423	8000.285060	9.501632	-0.054670	4.815631
272.565631	8000.272082	9.506637	-0.054656	4.815627
272.465203	8000.277910	9.511642	-0.054637	4.815630
272.430432	8000.290151	9.516647	-0.054630	4.815633
272.468050	8000.234154	9.521651	-0.054637	4.815617
272.388276	8000.244591	9.526656	-0.054622	4.815620
272.386681	8000.194361	9.531661	-0.054622	4.815606
272.522736	8000.270269	9.536666	-0.054647	4.815627
272.522275	8000.277730	9.541671	-0.054647	4.815629
272.523494	8000.209390	9.546675	-0.054647	4.815609
272.653745	8000.244619	9.551680	-0.054671	4.815619
272.450449	8000.209250	9.556685	-0.054633	4.815610
272.255581	8000.221011	9.561690	-0.054597	4.815614
272.271700	8000.289619	9.566695	-0.054600	4.815634
272.327554	8000.240328	9.571699	-0.054610	4.815619
272.574669	8000.307370	9.576704	-0.054656	4.815638
272.549598	8000.257825	9.581709	-0.054651	4.815623
272.603533	8000.240542	9.586714	-0.054661	4.815618
272.758135	8000.241992	9.591719	-0.054690	4.815618
272.577181	8000.260389	9.596723	-0.054656	4.815624
272.728183	8000.242556	9.601728	-0.054684	4.815618
272.566421	8000.204662	9.606733	-0.054654	4.815608
272.577745	8000.228335	9.611738	-0.054656	4.815615
272.567277	8000.265537	9.616743	-0.054654	4.815626
272.803718	8000.290753	9.621747	-0.054698	4.815632
272.714592	8000.241229	9.626752	-0.054681	4.815618
272.492423	8000.231184	9.631757	-0.054640	4.815616
272.696736	8000.259079	9.636762	-0.054678	4.815623
272.650090	8000.295690	9.641767	-0.054669	4.815634
272.643046	8000.245370	9.646771	-0.054668	4.815619
272.834926	8000.299763	9.651776	-0.054703	4.815634
272.851841	8000.253039	9.656781	-0.054706	4.815621
272.709476	8000.249637	9.661786	-0.054680	4.815620
272.567908	8000.310330	9.666791	-0.054653	4.815639
272.570852	8000.190753	9.671795	-0.054654	4.815604
272.593317	8000.219949	9.676800	-0.054658	4.815612
272.563082	8000.246148	9.681805	-0.054652	4.815620
272.600094	8000.221113	9.686810	-0.054659	4.815612
272.759426	8000.225844	9.691815	-0.054689	4.815613
272.707840	8000.206838	9.696819	-0.054679	4.815608
272.632019	8000.248312	9.701824	-0.054665	4.815620
272.530000	8000.259454	9.706829	-0.054646	4.815624
272.725918	8000.253035	9.711834	-0.054682	4.815621
272.633016	8000.226946	9.716839	-0.054665	4.815614
272.645227	8000.229274	9.721843	-0.054667	4.815615
272.731445	8000.330001	9.726848	-0.054683	4.815644
272.565767	8000.250389	9.731853	-0.054652	4.815621
272.723112	8000.216640	9.736858	-0.054681	4.815611
272.916916	8000.290288	9.741863	-0.054717	4.815631
272.674131	8000.257477	9.746867	-0.054672	4.815623
272.692543	8000.366709	9.751872	-0.054675	4.815655
272.754150	8000.305763	9.756877	-0.054687	4.815636
272.816356	8000.328132	9.761882	-0.054698	4.815643
272.711213	8000.341359	9.766887	-0.054679	4.815647
272.667785	8000.296853	9.771891	-0.054670	4.815634
273.084501	8000.298315	9.776896	-0.054748	4.815633
272.825623	8000.222520	9.781901	-0.054699	4.815612
272.851647	8000.207985	9.786906	-0.054704	4.815607
272.737148	8000.207175	9.791911	-0.054683	4.815608
272.741885	8000.233945	9.796915	-0.054684	4.815616
272.986739	8000.288136	9.801920	-0.054729	4.815630
272.984595	8000.312658	9.806925	-0.054729	4.815637
273.005794	8000.246779	9.811930	-0.054733	4.815618
272.882935	8000.246900	9.816935	-0.054710	4.815619
272.833923	8000.240752	9.821939	-0.054700	4.815617
272.753634	8000.278949	9.826944	-0.054685	4.815629
272.884894	8000.250114	9.831949	-0.054710	4.815620
273.102525	8000.237642	9.836954	-0.054750	4.815615
273.109299	8000.296487	9.841959	-0.054751	4.815632
272.986469	8000.220779	9.846963	-0.054728	4.815611
272.904641	8000.346529	9.851968	-0.054713	4.815648
272.806941	8000.269095	9.856973	-0.054695	4.815626
272.912315	8000.240905	9.861978	-0.054714	4.815617
272.860696	8000.276367	9.866983	-0.054705	4.815627
272.791625	8000.282707	9.871987	-0.054692	4.815630
272.995945	8000.353324	9.876992	-0.054730	4.815649
273.005881	8000.294737	9.881997	-0.054731	4.815632
273.100350	8000.268505	9.887002	-0.054749	4.815624
273.194235	8000.281780	9.892007	-0.054766	4.815627
273.134958	8000.214586	9.897011	-0.054755	4.815608
273.228619	8000.254558	9.902016	-0.054772	4.815619
273.158605	8000.230978	9.907021	-0.054759	4.815613
273.216010	8000.277834	9.912026	-0.054770	4.815626
273.156120	8000.303549	9.917031	-0.054759	4.815634
273.159681	8000.232041	9.922035	-0.054759	4.815613
273.213673	8000.273501	9.927040	-0.054769	4.815625
272.999753	8000.309515	9.932045	-0.054729	4.815636
273.149007	8000.282042	9.937050	-0.054757	4.815628
273.128576	8000.283837	9.942055	-0.054753	4.815628
273.173084	8000.280284	9.947059	-0.054761	4.815627
272.996562	8000.290209	9.952064	-0.054728	4.815631
272.990596	8000.253791	9.957069	-0.054727	4.815620
273.192932	8000.202620	9.962074	-0.054765	4.815604
273.064339	8000.268865	9.967079	-0.054741	4.815624
272.981291	8000.234392	9.972083	-0.054725	4.815615
273.036139	8000.352764	9.977088	-0.054735	4.815649
272.819277	8000.263771	9.982093	-0.054695	4.815624
273.126824	8000.243156	9.987098	-0.054752	4.815616
273.079905	8000.305395	9.992103	-0.054743	4.815635
273.061106	8000.207890	9.997107	-0.054740	4.815606
273.006410	8000.291363	10.002112	-0.054729	4.815631
272.915428	8000.278121	10.007117	-0.054712	4.815628
273.086766	8000.280913	10.012122	-0.054744	4.815628
273.139290	8000.299920	10.017127	-0.054754	4.815633
273.139712	8000.219818	10.022131	-0.054754	4.815610
273.074830	8000.234771	10.027136	-0.054742	4.815614
272.891598	8000.260606	10.032141	-0.054708	4.815623
272.828111	8000.243541	10.037146	-0.054696	4.815618
272.898411	8000.258566	10.042151	-0.054709	4.815622
273.055199	8000.234420	10.047155	-0.054738	4.815614
273.148766	8000.271186	10.052160	-0.054755	4.815625
273.038114	8000.234126	10.057165	-0.054734	4.815614
273.097790	8000.253250	10.062170	-0.054745	4.815620
273.219792	8000.302229	10.067175	-0.054768	4.815633
272.995164	8000.208837	10.072179	-0.054726	4.815607
273.366407	8000.305679	10.077184	-0.054795	4.815634
273.369860	8000.302524	10.082189	-0.054796	4.815633
273.244747	8000.250274	10.087194	-0.054772	4.815618
273.231087	8000.271404	10.092199	-0.054770	4.815624
273.181862	8000.169130	10.097203	-0.054760	4.815595
273.160044	8000.245663	10.102208	-0.054756	4.815617
273.135224	8000.274087	10.107213	-0.054752	4.815626
273.154051	8000.257299	10.112218	-0.054755	4.815621
273.029414	8000.241370	10.117223	-0.054732	4.815616
272.933607	8000.214165	10.122227	-0.054714	4.815609
273.132392	8000.279351	10.127232	-0.054751	4.815627
273.103635	8000.257513	10.132237	-0.054745	4.815621
273.002361	8000.257987	10.137242	-0.054726	4.815621
273.117919	8000.329290	10.142247	-0.054748	4.815642
273.142948	8000.277358	10.147251	-0.054752	4.815626
273.217039	8000.309534	10.152256	-0.054766	4.815636
273.083057	8000.238983	10.157261	-0.054741	4.815616
273.111775	8000.225561	10.162266	-0.054746	4.815611
273.054950	8000.266278	10.167271	-0.054736	4.815624
273.096554	8000.239182	10.172275	-0.054743	4.815616
273.269266	8000.298602	10.177280	-0.054775	4.815632
273.391432	8000.345449	10.182285	-0.054798	4.815645
273.383239	8000.308994	10.187290	-0.054796	4.815635
273.264639	8000.342293	10.192295	-0.054774	4.815645
273.274645	8000.218558	10.197299	-0.054776	4.815609
273.280056	8000.292333	10.202304	-0.054777	4.815630
273.100802	8000.274444	10.207309	-0.054744	4.815626
273.278681	8000.242098	10.212314	-0.054777	4.815616
273.436348	8000.266028	10.217319	-0.054806	4.815622
273.357113	8000.197440	10.222323	-0.054791	4.815602
273.171823	8000.332180	10.227328	-0.054756	4.815642
273.244406	8000.338699	10.232333	-0.054770	4.815644
273.184411	8000.237316	10.237338	-0.054759	4.815615
273.090334	8000.344710	10.242343	-0.054741	4.815646
273.383877	8000.283282	10.247347	-0.054796	4.815627
273.218118	8000.346784	10.252352	-0.054765	4.815646
272.957683	8000.259214	10.257357	-0.054716	4.815622
273.094677	8000.276398	10.262362	-0.054741	4.815626
273.303402	8000.308638	10.267367	-0.054780	4.815635
273.215626	8000.195053	10.272371	-0.054764	4.815602
273.296237	8000.250832	10.277376	-0.054779	4.815618
273.334376	8000.255720	10.282381	-0.054786	4.815619
273.343810	8000.213146	10.287386	-0.054787	4.815607
273.359509	8000.281749	10.292391	-0.054790	4.815627
273.270839	8000.229027	10.297395	-0.054774	4.815612
273.375974	8000.306568	10.302400	-0.054793	4.815634
273.222580	8000.250652	10.307405	-0.054764	4.815618
273.412132	8000.244130	10.312410	-0.054800	4.815616
273.582580	8000.336623	10.317415	-0.054831	4.815642
273.368652	8000.307486	10.322419	-0.054791	4.815634
273.364561	8000.341589	10.327424	-0.054791	4.815644
273.392378	8000.346309	10.332429	-0.054796	4.815646
273.325511	8000.269378	10.337434	-0.054783	4.815623
273.157646	8000.321097	10.342439	-0.054752	4.815639
273.152166	8000.272938	10.347443	-0.054751	4.815625
273.252847	8000.238263	10.352448	-0.054769	4.815615
273.085172	8000.287849	10.357453	-0.054738	4.815630
273.240118	8000.228428	10.362458	-0.054767	4.815612
273.602091	8000.331527	10.367463	-0.054834	4.815640
273.366573	8000.295629	10.372467	-0.054790	4.815631
273.300594	8000.272115	10.377472	-0.054778	4.815624
273.322520	8000.298099	10.382477	-0.054782	4.815632
273.536170	8000.233229	10.387482	-0.054822	4.815612
273.584532	8000.258577	10.392487	-0.054830	4.815619
273.526146	8000.228778	10.397491	-0.054819	4.815611
273.462922	8000.264050	10.402496	-0.054808	4.815621
273.388174	8000.245733	10.407501	-0.054794	4.815616
273.501471	8000.251849	10.412506	-0.054815	4.815617
273.529247	8000.320650	10.417511	-0.054820	4.815637
273.382469	8000.305427	10.422515	-0.054792	4.815634
273.463739	8000.255482	10.427520	-0.054807	4.815619
273.420779	8000.227004	10.432525	-0.054799	4.815611
273.330452	8000.303486	10.437530	-0.054782	4.815633
273.218688	8000.306993	10.442535	-0.054762	4.815635
273.440912	8000.307413	10.447539	-0.054803	4.815634
273.409819	8000.301557	10.452544	-0.054797	4.815632
273.344652	8000.263104	10.457549	-0.054785	4.815621
273.341040	8000.175459	10.462554	-0.054784	4.815596
273.483172	8000.206611	10.467559	-0.054810	4.815604
273.480402	8000.237531	10.472563	-0.054810	4.815613
273.376453	8000.298838	10.477568	-0.054790	4.815632
273.579306	8000.376909	10.482573	-0.054828	4.815654
273.405553	8000.239489	10.487578	-0.054795	4.815614
273.396904	8000.266041	10.492583	-0.054794	4.815622
273.275952	8000.192499	10.497587	-0.054771	4.815601
273.384119	8000.317083	10.502592	-0.054791	4.815637
273.310599	8000.299854	10.507597	-0.054778	4.815632
273.273335	8000.245836	10.512602	-0.054770	4.815617
273.393185	8000.303324	10.517607	-0.054793	4.815633
273.439807	8000.212228	10.522611	-0.054801	4.815606
273.579095	8000.217701	10.527616	-0.054827	4.815607
273.705917	8000.229379	10.532621	-0.054851	4.815610
273.693798	8000.214221	10.537626	-0.054848	4.815606
273.584456	8000.229515	10.542631	-0.054828	4.815611
273.510962	8000.204809	10.547635	-0.054814	4.815604
273.591716	8000.287292	10.552640	-0.054829	4.815627
273.678213	8000.292971	10.557645	-0.054845	4.815629
273.528976	8000.201877	10.562650	-0.054817	4.815603
273.519957	8000.326683	10.567655	-0.054815	4.815639
273.564371	8000.215257	10.572659	-0.054824	4.815606
273.614500	8000.274811	10.577664	-0.054833	4.815624
273.615133	8000.359189	10.582669	-0.054833	4.815648
273.618054	8000.246017	10.587674	-0.054833	4.815615
273.558703	8000.259992	10.592679	-0.054822	4.815620
273.257196	8000.237969	10.597683	-0.054766	4.815615
273.472818	8000.275662	10.602688	-0.054806	4.815625
273.498134	8000.268592	10.607693	-0.054811	4.815622
273.453857	8000.234752	10.612698	-0.054802	4.815613
273.507336	8000.310381	10.617703	-0.054812	4.815635
273.394229	8000.211334	10.622707	-0.054791	4.815606
273.542195	8000.289575	10.627712	-0.054819	4.815628
273.614296	8000.239481	10.632717	-0.054832	4.815613
273.693638	8000.223681	10.637722	-0.054847	4.815608
273.655139	8000.252950	10.642727	-0.054839	4.815617
273.672758	8000.184876	10.647731	-0.054842	4.815597
273.852034	8000.307419	10.652736	-0.054876	4.815632
273.729851	8000.286190	10.657741	-0.054853	4.815626
273.586135	8000.272085	10.662746	-0.054826	4.815623
273.683137	8000.255506	10.667751	-0.054844	4.815618
273.682744	8000.266173	10.672755	-0.054844	4.815621
273.765166	8000.298486	10.677760	-0.054859	4.815630
273.553327	8000.286471	10.682765	-0.054820	4.815627
273.437719	8000.198064	10.687770	-0.054798	4.815602
273.471296	8000.286184	10.692775	-0.054804	4.815628
273.391297	8000.181270	10.697779	-0.054789	4.815597
273.553104	8000.265077	10.702784	-0.054819	4.815621
273.567452	8000.285597	10.707789	-0.054822	4.815627
273.610358	8000.230753	10.712794	-0.054830	4.815611
273.525790	8000.330827	10.717799	-0.054814	4.815641
273.764278	8000.265295	10.722803	-0.054858	4.815620
273.629914	8000.326105	10.727808	-0.054833	4.815639
273.586195	8000.327519	10.732813	-0.054825	4.815639
273.655193	8000.258149	10.737818	-0.054838	4.815619
273.778097	8000.311416	10.742823	-0.054861	4.815634
273.624418	8000.231998	10.747827	-0.054832	4.815611
273.744504	8000.229681	10.752832	-0.054854	4.815610
273.698823	8000.170185	10.757837	-0.054845	4.815593
273.421091	8000.211565	10.762842	-0.054794	4.815606
273.489993	8000.304534	10.767847	-0.054807	4.815633
273.487915	8000.227594	10.772851	-0.054806	4.815611
273.666850	8000.223035	10.777856	-0.054839	4.815608
273.516008	8000.268624	10.782861	-0.054811	4.815622
273.585972	8000.222766	10.787866	-0.054824	4.815609
273.892856	8000.308946	10.792871	-0.054881	4.815632
273.542926	8000.281858	10.797875	-0.054816	4.815626
273.649703	8000.264371	10.802880	-0.054836	4.815621
273.757795	8000.245837	10.807885	-0.054856	4.815615
273.704034	8000.211842	10.812890	-0.054846	4.815605
273.782231	8000.261174	10.817895	-0.054860	4.815619
273.588602	8000.211009	10.822899	-0.054824	4.815605
273.608979	8000.185701	10.827904	-0.054828	4.815598
273.516343	8000.278167	10.832909	-0.054810	4.815625
273.692580	8000.228706	10.837914	-0.054843	4.815610
273.857792	8000.327523	10.842919	-0.054874	4.815638
273.619441	8000.285170	10.847923	-0.054829	4.815627
273.583379	8000.239715	10.852928	-0.054822	4.815614
273.760798	8000.286397	10.857933	-0.054855	4.815626
273.708314	8000.217177	10.862938	-0.054845	4.815606
273.807405	8000.240150	10.867943	-0.054864	4.815613
273.959402	8000.214858	10.872947	-0.054892	4.815605
273.777880	8000.238585	10.877952	-0.054858	4.815612
273.565839	8000.261813	10.882957	-0.054819	4.815620
273.572492	8000.235213	10.887962	-0.054820	4.815612
273.743568	8000.312765	10.892967	-0.054852	4.815634
273.758964	8000.206205	10.897971	-0.054854	4.815603
273.767822	8000.268288	10.902976	-0.054856	4.815621
273.901863	8000.298241	10.907981	-0.054881	4.815629
273.703934	8000.219167	10.912986	-0.054844	4.815607
273.827437	8000.303418	10.917991	-0.054867	4.815631
273.956186	8000.258521	10.922995	-0.054891	4.815617
274.051538	8000.212010	10.928000	-0.054908	4.815603
273.765135	8000.290629	10.933005	-0.054855	4.815628
273.870090	8000.225050	10.938010	-0.054874	4.815608
274.077224	8000.255129	10.943015	-0.054913	4.815616
273.911809	8000.265235	10.948019	-0.054882	4.815620
273.723749	8000.263221	10.953024	-0.054847	4.815620
273.788657	8000.262139	10.958029	-0.054859	4.815619
273.717734	8000.243883	10.963034	-0.054846	4.815614
273.891052	8000.287294	10.968039	-0.054878	4.815626
273.703961	8000.247915	10.973043	-0.054843	4.815616
273.950996	8000.217768	10.978048	-0.054889	4.815606
273.902300	8000.286388	10.983053	-0.054880	4.815626
273.860579	8000.345509	10.988058	-0.054872	4.815643
274.002543	8000.364911	10.993063	-0.054898	4.815648
273.928454	8000.315630	10.998067	-0.054884	4.815634
273.911036	8000.257664	11.003072	-0.054881	4.815617
273.791256	8000.246086	11.008077	-0.054858	4.815615
273.672985	8000.252690	11.013082	-0.054836	4.815617
273.728552	8000.323013	11.018087	-0.054847	4.815637
273.687381	8000.292428	11.023091	-0.054839	4.815629
273.813312	8000.274186	11.028096	-0.054862	4.815623
273.625416	8000.247610	11.033101	-0.054827	4.815616
273.521602	8000.255519	11.038106	-0.054808	4.815619
273.739132	8000.331693	11.043111	-0.054848	4.815640
273.708448	8000.239333	11.048115	-0.054842	4.815613
273.708556	8000.293797	11.053120	-0.054842	4.815629
273.670506	8000.277147	11.058125	-0.054835	4.815624
273.647239	8000.213745	11.063130	-0.054831	4.815606
273.901905	8000.286255	11.068135	-0.054878	4.815626
273.760288	8000.256163	11.073139	-0.054852	4.815618
273.979604	8000.264013	11.078144	-0.054892	4.815619
273.811368	8000.309317	11.083149	-0.054861	4.815633
273.795159	8000.250303	11.088154	-0.054858	4.815616
273.733708	8000.317645	11.093159	-0.054846	4.815636
273.698888	8000.306388	11.098163	-0.054840	4.815633
273.682806	8000.278349	11.103168	-0.054837	4.815625
273.698404	8000.301025	11.108173	-0.054840	4.815631
273.812760	8000.289003	11.113178	-0.054861	4.815627
273.811600	8000.369080	11.118183	-0.054860	4.815651
273.747465	8000.275104	11.123187	-0.054848	4.815623
273.780701	8000.243598	11.128192	-0.054854	4.815614
273.804117	8000.315533	11.133197	-0.054859	4.815635
273.662784	8000.271561	11.138202	-0.054832	4.815623
273.873769	8000.294227	11.143207	-0.054872	4.815628
273.860023	8000.235253	11.148211	-0.054869	4.815611
273.788730	8000.247965	11.153216	-0.054856	4.815615
273.762413	8000.299861	11.158221	-0.054851	4.815631
273.827466	8000.264603	11.163226	-0.054863	4.815620
273.901034	8000.259390	11.168231	-0.054876	4.815618
273.760794	8000.232526	11.173235	-0.054850	4.815611
273.801657	8000.304745	11.178240	-0.054858	4.815632
273.956985	8000.323297	11.183245	-0.054886	4.815636
273.962175	8000.273176	11.188250	-0.054887	4.815622
274.067632	8000.371017	11.193255	-0.054907	4.815650
274.094277	8000.306294	11.198259	-0.054912	4.815631
273.790431	8000.331225	11.203264	-0.054855	4.815640
273.625705	8000.316777	11.208269	-0.054824	4.815636
273.816091	8000.251526	11.213274	-0.054860	4.815616
274.003350	8000.286621	11.218279	-0.054894	4.815626
273.874775	8000.325098	11.223283	-0.054870	4.815637
274.001762	8000.342119	11.228288	-0.054894	4.815642
273.877106	8000.346482	11.233293	-0.054871	4.815644
273.836036	8000.242203	11.238298	-0.054863	4.815613
273.858426	8000.285283	11.243303	-0.054867	4.815626
273.770797	8000.227237	11.248307	-0.054851	4.815609
273.779146	8000.210278	11.253312	-0.054852	4.815604
273.880194	8000.250371	11.258317	-0.054871	4.815616
273.863674	8000.205236	11.263322	-0.054868	4.815602
273.886933	8000.336978	11.268327	-0.054872	4.815641
273.722813	8000.261661	11.273331	-0.054841	4.815620
273.860114	8000.258557	11.278336	-0.054867	4.815618
273.834249	8000.278420	11.283341	-0.054862	4.815624
273.771103	8000.186597	11.288346	-0.054850	4.815597
273.882686	8000.225795	11.293351	-0.054871	4.815608
273.972668	8000.253959	11.298355	-0.054887	4.815616
273.940760	8000.234205	11.303360	-0.054881	4.815611
273.807268	8000.277942	11.308365	-0.054856	4.815624
273.864219	8000.222259	11.313370	-0.054867	4.815607
273.858227	8000.305461	11.318375	-0.054866	4.815632
273.909434	8000.289202	11.323379	-0.054875	4.815627
274.141930	8000.303675	11.328384	-0.054918	4.815630
274.045641	8000.317046	11.333389	-0.054900	4.815634
273.972125	8000.283796	11.338394	-0.054887	4.815625
273.998123	8000.351500	11.343399	-0.054891	4.815645
273.736109	8000.280991	11.348403	-0.054842	4.815625
273.646871	8000.293410	11.353408	-0.054826	4.815629
273.616224	8000.317466	11.358413	-0.054820	4.815636
273.812905	8000.227754	11.363418	-0.054856	4.815609
274.023033	8000.233317	11.368423	-0.054896	4.815610
273.653182	8000.261442	11.373427	-0.054827	4.815620
273.886169	8000.240677	11.378432	-0.054870	4.815613
273.955343	8000.248209	11.383437	-0.054883	4.815615
273.772698	8000.218515	11.388442	-0.054849	4.815607
273.784045	8000.288116	11.393447	-0.054851	4.815627
273.776948	8000.252747	11.398451	-0.054849	4.815617
274.019418	8000.284472	11.403456	-0.054894	4.815625
273.900870	8000.332725	11.408461	-0.054872	4.815640
273.888991	8000.301550	11.413466	-0.054870	4.815631
274.026303	8000.265337	11.418471	-0.054895	4.815619
273.787106	8000.247536	11.423475	-0.054851	4.815615
273.848814	8000.217564	11.428480	-0.054862	4.815606
274.022300	8000.302631	11.433485	-0.054894	4.815630
273.822624	8000.258774	11.438490	-0.054857	4.815618
273.761633	8000.314376	11.443495	-0.054846	4.815635
273.907433	8000.300731	11.448499	-0.054873	4.815630
273.983549	8000.278471	11.453504	-0.054887	4.815623
273.770759	8000.283530	11.458509	-0.054847	4.815626
273.764135	8000.233216	11.463514	-0.054846	4.815611
273.940469	8000.305513	11.468519	-0.054878	4.815631
273.752779	8000.280009	11.473523	-0.054843	4.815625
273.783328	8000.215351	11.478528	-0.054849	4.815606
273.777523	8000.237677	11.483533	-0.054848	4.815612
273.990446	8000.193088	11.488538	-0.054887	4.815598
274.032829	8000.265332	11.493543	-0.054895	4.815619
274.034969	8000.255747	11.498547	-0.054896	4.815616
274.230617	8000.229033	11.503552	-0.054932	4.815608
274.063054	8000.231626	11.508557	-0.054901	4.815609
273.819289	8000.224431	11.513562	-0.054855	4.815608
274.044951	8000.245200	11.518567	-0.054897	4.815613
274.067046	8000.275459	11.523571	-0.054901	4.815622
274.033809	8000.283453	11.528576	-0.054895	4.815625
274.068104	8000.271189	11.533581	-0.054901	4.815621
274.083167	8000.244727	11.538586	-0.054904	4.815613
274.060076	8000.340466	11.543591	-0.054900	4.815641
274.029395	8000.329277	11.548595	-0.054894	4.815638
274.023103	8000.266152	11.553600	-0.054892	4.815620
274.015233	8000.294853	11.558605	-0.054891	4.815628
273.893270	8000.218089	11.563610	-0.054868	4.815606
274.199159	8000.244442	11.568615	-0.054925	4.815612
273.958930	8000.244780	11.573619	-0.054880	4.815614
274.007513	8000.259451	11.578624	-0.054889	4.815618
273.970557	8000.312242	11.583629	-0.054882	4.815633
274.050486	8000.240914	11.588634	-0.054897	4.815612
274.052492	8000.292206	11.593639	-0.054897	4.815627
273.693172	8000.320502	11.598643	-0.054830	4.815637
273.994469	8000.296583	11.603648	-0.054886	4.815629
274.112653	8000.343365	11.608653	-0.054908	4.815642
273.792161	8000.281512	11.613658	-0.054848	4.815625
274.018550	8000.356765	11.618663	-0.054891	4.815646
274.139590	8000.351260	11.623667	-0.054913	4.815644
273.994159	8000.325377	11.628672	-0.054886	4.815637
274.118818	8000.326340	11.633677	-0.054909	4.815637
274.092048	8000.275696	11.638682	-0.054904	4.815622
273.939784	8000.308446	11.643687	-0.054875	4.815632
273.849764	8000.342212	11.648691	-0.054859	4.815643
274.070048	8000.275314	11.653696	-0.054899	4.815622
274.047104	8000.351831	11.658701	-0.054895	4.815645
273.989556	8000.254759	11.663706	-0.054884	4.815616
274.100870	8000.348423	11.668711	-0.054905	4.815643
273.897694	8000.308781	11.673715	-0.054867	4.815633
273.838784	8000.323831	11.678720	-0.054856	4.815637
273.926476	8000.392544	11.683725	-0.054872	4.815657
274.087492	8000.283024	11.688730	-0.054902	4.815624
274.097592	8000.371830	11.693735	-0.054904	4.815650
273.943771	8000.347946	11.698739	-0.054875	4.815644
273.969069	8000.316311	11.703744	-0.054880	4.815635
274.032825	8000.375021	11.708749	-0.054892	4.815651
274.014014	8000.265765	11.713754	-0.054888	4.815620
274.082066	8000.279686	11.718759	-0.054901	4.815623
274.226287	8000.327963	11.723763	-0.054927	4.815637
274.037366	8000.339819	11.728768	-0.054892	4.815641
273.994096	8000.370078	11.733773	-0.054884	4.815650
274.100518	8000.304523	11.738778	-0.054904	4.815631
273.952502	8000.396084	11.743783	-0.054876	4.815658
273.927782	8000.320909	11.748787	-0.054871	4.815636
274.055270	8000.254631	11.753792	-0.054895	4.815616
273.970961	8000.310920	11.758797	-0.054879	4.815633
273.963584	8000.333221	11.763802	-0.054878	4.815640
274.191586	8000.321988	11.768807	-0.054920	4.815635
274.243597	8000.292925	11.773811	-0.054930	4.815626
274.078006	8000.263510	11.778816	-0.054899	4.815619
274.161477	8000.355651	11.783821	-0.054914	4.815645
274.166547	8000.257466	11.788826	-0.054915	4.815616
274.088521	8000.314926	11.793831	-0.054901	4.815634
273.869429	8000.294248	11.798835	-0.054860	4.815629
274.137706	8000.250564	11.803840	-0.054909	4.815615
273.969159	8000.287319	11.808845	-0.054878	4.815626
274.071124	8000.245188	11.813850	-0.054897	4.815613
274.288902	8000.333117	11.818855	-0.054937	4.815638
274.245354	8000.315309	11.823859	-0.054929	4.815633
274.177930	8000.233027	11.828864	-0.054917	4.815609
274.144050	8000.312570	11.833869	-0.054910	4.815633
274.052200	8000.248046	11.838874	-0.054893	4.815614
274.004323	8000.359401	11.843879	-0.054884	4.815647
273.896724	8000.280735	11.848883	-0.054864	4.815625
274.118753	8000.217070	11.853888	-0.054905	4.815605
274.225744	8000.273282	11.858893	-0.054925	4.815621
273.995788	8000.250291	11.863898	-0.054882	4.815615
274.126431	8000.322910	11.868903	-0.054906	4.815636
274.165089	8000.284016	11.873907	-0.054913	4.815624
274.092318	8000.359719	11.878912	-0.054900	4.815647
274.235004	8000.300097	11.883917	-0.054926	4.815629
274.247510	8000.270389	11.888922	-0.054929	4.815620
274.292101	8000.340534	11.893927	-0.054937	4.815640
274.149945	8000.322181	11.898931	-0.054910	4.815636
274.256794	8000.284403	11.903936	-0.054930	4.815624
274.359219	8000.327724	11.908941	-0.054949	4.815636
274.056151	8000.242658	11.913946	-0.054892	4.815613
274.240827	8000.334318	11.918951	-0.054927	4.815639
274.227365	8000.313797	11.923955	-0.054924	4.815633
274.156468	8000.288066	11.928960	-0.054911	4.815626
273.975055	8000.333155	11.933965	-0.054877	4.815640
274.005375	8000.258880	11.938970	-0.054883	4.815618
274.200586	8000.372073	11.943975	-0.054919	4.815650
274.082917	8000.348780	11.948979	-0.054897	4.815644
274.107807	8000.298981	11.953984	-0.054901	4.815629
274.265388	8000.325047	11.958989	-0.054931	4.815636
274.097641	8000.282780	11.963994	-0.054899	4.815624
274.202017	8000.337881	11.968999	-0.054919	4.815640
274.115428	8000.319369	11.974003	-0.054903	4.815635
274.023929	8000.274076	11.979008	-0.054885	4.815622
274.116434	8000.307622	11.984013	-0.054903	4.815631
274.131489	8000.290772	11.989018	-0.054905	4.815626
274.308957	8000.316095	11.994023	-0.054938	4.815633
274.001417	8000.296107	11.999027	-0.054881	4.815629
274.180449	8000.338544	12.004032	-0.054914	4.815640
274.306310	8000.325642	12.009037	-0.054937	4.815636
274.091255	8000.281533	12.014042	-0.054897	4.815624
273.912398	8000.299962	12.019047	-0.054864	4.815630
274.138858	8000.339971	12.024051	-0.054906	4.815641
274.116923	8000.277658	12.029056	-0.054902	4.815623
274.151401	8000.347637	12.034061	-0.054908	4.815643
274.058911	8000.368547	12.039066	-0.054891	4.815650
274.323925	8000.329082	12.044071	-0.054940	4.815637
274.240911	8000.344806	12.049075	-0.054925	4.815642
274.285452	8000.301737	12.054080	-0.054933	4.815629
274.375932	8000.397198	12.059085	-0.054950	4.815656
274.251249	8000.304367	12.064090	-0.054926	4.815630
274.113816	8000.313861	12.069095	-0.054901	4.815633
274.194064	8000.316233	12.074099	-0.054915	4.815634
274.221529	8000.279293	12.079104	-0.054920	4.815623
274.009293	8000.350580	12.084109	-0.054881	4.815645
274.070746	8000.288562	12.089114	-0.054892	4.815626
274.214832	8000.307999	12.094119	-0.054919	4.815631
274.149183	8000.332551	12.099123	-0.054907	4.815639
274.060322	8000.252056	12.104128	-0.054890	4.815616
274.250484	8000.303219	12.109133	-0.054925	4.815630
274.161849	8000.315647	12.114138	-0.054909	4.815634
274.073898	8000.304589	12.119143	-0.054892	4.815631
274.139626	8000.368672	12.124147	-0.054904	4.815649
274.077976	8000.335615	12.129152	-0.054893	4.815640
274.100906	8000.389385	12.134157	-0.054897	4.815656
274.397232	8000.348296	12.139162	-0.054952	4.815642
274.323289	8000.332126	12.144167	-0.054938	4.815638
274.172256	8000.297608	12.149171	-0.054910	4.815628
274.226049	8000.261098	12.154176	-0.054920	4.815617
274.373844	8000.351088	12.159181	-0.054948	4.815643
274.289942	8000.320871	12.164186	-0.054932	4.815635
274.212755	8000.303581	12.169191	-0.054917	4.815630
274.251361	8000.294592	12.174195	-0.054924	4.815627
274.376839	8000.256050	12.179200	-0.054948	4.815615
274.204479	8000.341873	12.184205	-0.054916	4.815641
274.253032	8000.252943	12.189210	-0.054924	4.815615
274.371946	8000.285853	12.194215	-0.054947	4.815624
274.247863	8000.298770	12.199219	-0.054923	4.815628
274.225812	8000.254612	12.204224	-0.054919	4.815616
274.322309	8000.329877	12.209229	-0.054937	4.815637
274.293125	8000.332597	12.214234	-0.054932	4.815638
274.282912	8000.386893	12.219239	-0.054930	4.815654
274.223834	8000.322905	12.224243	-0.054918	4.815636
274.423431	8000.305868	12.229248	-0.054956	4.815630
274.487848	8000.325070	12.234253	-0.054967	4.815635
274.225239	8000.215032	12.239258	-0.054918	4.815604
274.233341	8000.305942	12.244263	-0.054920	4.815631
274.233430	8000.313412	12.249267	-0.054920	4.815633
274.125012	8000.296679	12.254272	-0.054900	4.815628
274.207910	8000.357838	12.259277	-0.054915	4.815646
274.215948	8000.287471	12.264282	-0.054916	4.815625
274.405657	8000.318334	12.269287	-0.054952	4.815633
274.363704	8000.331525	12.274291	-0.054944	4.815637
274.278987	8000.242553	12.279296	-0.054928	4.815612
274.293021	8000.375213	12.284301	-0.054930	4.815651
274.043454	8000.326267	12.289306	-0.054884	4.815637
274.382066	8000.292278	12.294311	-0.054947	4.815626
274.324762	8000.327647	12.299315	-0.054936	4.815636
274.026230	8000.264017	12.304320	-0.054880	4.815619
274.126552	8000.376726	12.309325	-0.054899	4.815652
274.185569	8000.337098	12.314330	-0.054910	4.815640
274.194801	8000.367147	12.319335	-0.054911	4.815649
274.134788	8000.368294	12.324339	-0.054900	4.815649
274.244701	8000.263279	12.329344	-0.054921	4.815618
274.366673	8000.283422	12.334349	-0.054943	4.815623
274.080618	8000.247765	12.339354	-0.054890	4.815614
274.243958	8000.230135	12.344359	-0.054920	4.815608
274.216328	8000.260649	12.349363	-0.054915	4.815617
274.171519	8000.221459	12.354368	-0.054906	4.815606
274.251925	8000.343456	12.359373	-0.054921	4.815641
274.324018	8000.288020	12.364378	-0.054935	4.815625
274.346801	8000.278773	12.369383	-0.054939	4.815622
274.151174	8000.312949	12.374387	-0.054902	4.815633
274.376185	8000.280306	12.379392	-0.054944	4.815622
274.362181	8000.332404	12.384397	-0.054941	4.815638
274.042298	8000.275901	12.389402	-0.054882	4.815623
274.433644	8000.310061	12.394407	-0.054955	4.815631
274.370166	8000.373099	12.399411	-0.054943	4.815650
274.257219	8000.250555	12.404416	-0.054922	4.815614
274.223593	8000.362143	12.409421	-0.054915	4.815647
274.092938	8000.299121	12.414426	-0.054891	4.815629
274.190700	8000.297507	12.419431	-0.054909	4.815628
274.032755	8000.284237	12.424435	-0.054879	4.815625
274.332865	8000.277387	12.429440	-0.054935	4.815622
274.444620	8000.304840	12.434445	-0.054956	4.815629
274.210237	8000.244394	12.439450	-0.054912	4.815613
274.242773	8000.263076	12.444455	-0.054918	4.815618
274.416697	8000.312906	12.449459	-0.054951	4.815632
274.324887	8000.288968	12.454464	-0.054933	4.815625
274.362558	8000.270352	12.459469	-0.054940	4.815620
274.160176	8000.265968	12.464474	-0.054902	4.815619
274.406687	8000.280671	12.469479	-0.054948	4.815622
274.345978	8000.338414	12.474483	-0.054937	4.815640
274.503918	8000.291858	12.479488	-0.054966	4.815625
274.445390	8000.317595	12.484493	-0.054955	4.815633
274.340740	8000.316945	12.489498	-0.054936	4.815633
274.345324	8000.350122	12.494503	-0.054937	4.815643
274.383231	8000.353938	12.499507	-0.054943	4.815644
274.223990	8000.216753	12.504512	-0.054914	4.815605
274.239704	8000.273609	12.509517	-0.054917	4.815621
274.140242	8000.220709	12.514522	-0.054898	4.815606
274.431284	8000.267114	12.519527	-0.054952	4.815618
274.111132	8000.257600	12.524531	-0.054892	4.815617
274.216866	8000.253981	12.529536	-0.054912	4.815616
274.399244	8000.283656	12.534541	-0.054946	4.815623
274.543737	8000.186682	12.539546	-0.054973	4.815594
274.515486	8000.259908	12.544551	-0.054967	4.815616
274.284538	8000.310596	12.549555	-0.054924	4.815632
274.371754	8000.313082	12.554560	-0.054940	4.815632
274.448290	8000.335687	12.559565	-0.054955	4.815638
274.446945	8000.273711	12.564570	-0.054954	4.815620
274.375435	8000.273602	12.569575	-0.054941	4.815621
274.220196	8000.310575	12.574579	-0.054912	4.815632
274.179369	8000.226592	12.579584	-0.054904	4.815608
274.230733	8000.315004	12.584589	-0.054914	4.815633
274.138194	8000.252605	12.589594	-0.054896	4.815616
274.147741	8000.275183	12.594599	-0.054898	4.815622
274.327357	8000.255683	12.599603	-0.054931	4.815616
274.363395	8000.239176	12.604608	-0.054938	4.815611
274.419366	8000.306302	12.609613	-0.054948	4.815630
274.259988	8000.283396	12.614618	-0.054919	4.815624
274.591014	8000.223649	12.619623	-0.054980	4.815605
274.465284	8000.280329	12.624627	-0.054957	4.815622
274.289708	8000.192008	12.629632	-0.054924	4.815597
274.466593	8000.279268	12.634637	-0.054957	4.815622
274.375760	8000.290592	12.639642	-0.054940	4.815626
274.425298	8000.279646	12.644647	-0.054949	4.815622
274.316364	8000.298151	12.649651	-0.054928	4.815628
274.362773	8000.350168	12.654656	-0.054937	4.815643
274.444892	8000.364320	12.659661	-0.054952	4.815647
274.338757	8000.309175	12.664666	-0.054932	4.815631
274.394162	8000.283372	12.669671	-0.054943	4.815623
274.200216	8000.376318	12.674675	-0.054906	4.815651
274.254611	8000.362247	12.679680	-0.054916	4.815647
274.347737	8000.375511	12.684685	-0.054934	4.815651
274.310944	8000.343929	12.689690	-0.054927	4.815641
274.450307	8000.298137	12.694695	-0.054953	4.815627
274.444468	8000.315123	12.699699	-0.054951	4.815632
274.471836	8000.261092	12.704704	-0.054956	4.815616
274.451320	8000.309880	12.709709	-0.054953	4.815631
274.387881	8000.226595	12.714714	-0.054941	4.815607
274.622447	8000.315867	12.719719	-0.054984	4.815632
274.507593	8000.349228	12.724723	-0.054963	4.815642
274.384302	8000.262828	12.729728	-0.054940	4.815617
274.436385	8000.325619	12.734733	-0.054949	4.815636
274.749017	8000.266640	12.739738	-0.055007	4.815617
274.434774	8000.260427	12.744743	-0.054949	4.815616
274.469485	8000.346431	12.749747	-0.054955	4.815641
274.449634	8000.309785	12.754752	-0.054951	4.815631
274.589978	8000.372952	12.759757	-0.054978	4.815649
274.557067	8000.317935	12.764762	-0.054971	4.815633
274.569730	8000.355517	12.769767	-0.054974	4.815644
274.391187	8000.306664	12.774771	-0.054940	4.815630
274.430179	8000.292341	12.779776	-0.054947	4.815626
274.484975	8000.365857	12.784781	-0.054958	4.815647
274.452224	8000.302299	12.789786	-0.054951	4.815629
274.484565	8000.301752	12.794791	-0.054957	4.815628
274.554462	8000.290071	12.799795	-0.054970	4.815625
274.621720	8000.261258	12.804800	-0.054983	4.815616
274.615567	8000.293191	12.809805	-0.054981	4.815625
274.521422	8000.315142	12.814810	-0.054964	4.815632
274.688389	8000.413990	12.819815	-0.054995	4.815660
274.488799	8000.367996	12.824819	-0.054958	4.815648
274.476467	8000.361379	12.829824	-0.054955	4.815646
274.485639	8000.408516	12.834829	-0.054957	4.815660
274.482791	8000.327290	12.839834	-0.054956	4.815636
274.381872	8000.353402	12.844839	-0.054937	4.815644
274.282810	8000.358183	12.849843	-0.054919	4.815646
274.406073	8000.316400	12.854848	-0.054942	4.815633
274.579069	8000.339515	12.859853	-0.054974	4.815639
274.399239	8000.314138	12.864858	-0.054940	4.815632
274.530552	8000.330162	12.869863	-0.054965	4.815636
274.764582	8000.288054	12.874867	-0.055008	4.815623
274.630914	8000.254888	12.879872	-0.054983	4.815614
274.572700	8000.280630	12.884877	-0.054972	4.815622
274.605465	8000.331357	12.889882	-0.054978	4.815636
274.644127	8000.313825	12.894887	-0.054985	4.815631
274.490231	8000.303824	12.899891	-0.054957	4.815629
274.579453	8000.279642	12.904896	-0.054973	4.815621
274.781985	8000.344894	12.909901	-0.055011	4.815640
274.540659	8000.329192	12.914906	-0.054966	4.815636
274.564621	8000.327440	12.919911	-0.054970	4.815636
274.601561	8000.300267	12.924915	-0.054977	4.815627
274.488637	8000.268508	12.929920	-0.054956	4.815619
274.485269	8000.320780	12.934925	-0.054955	4.815634
274.606417	8000.261874	12.939930	-0.054978	4.815616
274.536909	8000.273547	12.944935	-0.054964	4.815620
274.649940	8000.280728	12.949939	-0.054985	4.815621
274.711225	8000.266769	12.954944	-0.054997	4.815617
274.753735	8000.369991	12.959949	-0.055005	4.815647
274.519636	8000.288187	12.964954	-0.054961	4.815624
274.676989	8000.319590	12.969959	-0.054990	4.815633
274.850576	8000.330966	12.974963	-0.055022	4.815635
274.585837	8000.223028	12.979968	-0.054973	4.815605
274.711484	8000.293430	12.984973	-0.054996	4.815625
274.690291	8000.288804	12.989978	-0.054992	4.815624
274.787215	8000.361942	12.994983	-0.055010	4.815645
274.809814	8000.307833	12.999987	-0.055014	4.815629
274.746507	8000.246979	13.004992	-0.055002	4.815611
274.633771	8000.333777	13.009997	-0.054981	4.815637
274.474358	8000.253195	13.015002	-0.054952	4.815614
274.530618	8000.312850	13.020007	-0.054962	4.815631
274.721364	8000.346936	13.025011	-0.054998	4.815641
274.488121	8000.252330	13.030016	-0.054954	4.815614
274.589484	8000.292429	13.035021	-0.054973	4.815625
274.671801	8000.302312	13.040026	-0.054988	4.815628
274.650566	8000.264575	13.045031	-0.054984	4.815617
274.450647	8000.290137	13.050035	-0.054947	4.815625
274.685777	8000.233095	13.055040	-0.054990	4.815607
274.818038	8000.360213	13.060045	-0.055015	4.815644
274.623571	8000.332460	13.065050	-0.054979	4.815637
274.801285	8000.257390	13.070055	-0.055012	4.815614
274.842698	8000.337096	13.075059	-0.055019	4.815637
274.714659	8000.230325	13.080064	-0.054995	4.815606
274.850736	8000.277401	13.085069	-0.055021	4.815620
274.739807	8000.244606	13.090074	-0.055000	4.815611
274.684156	8000.249029	13.095079	-0.054989	4.815612
274.553221	8000.325917	13.100083	-0.054965	4.815635
274.484349	8000.313035	13.105088	-0.054952	4.815632
274.742971	8000.333277	13.110093	-0.055000	4.815636
274.621843	8000.294975	13.115098	-0.054977	4.815626
274.651217	8000.244181	13.120103	-0.054983	4.815611
274.750117	8000.291717	13.125107	-0.055001	4.815624
274.724526	8000.293427	13.130112	-0.054996	4.815625
274.750191	8000.329086	13.135117	-0.055001	4.815635
274.706371	8000.344383	13.140122	-0.054993	4.815640
274.737151	8000.273318	13.145127	-0.054998	4.815619
274.660027	8000.252825	13.150131	-0.054984	4.815613
274.496206	8000.249071	13.155136	-0.054953	4.815613
274.674083	8000.337417	13.160141	-0.054986	4.815638
274.678023	8000.277662	13.165146	-0.054987	4.815621
274.639741	8000.297322	13.170151	-0.054980	4.815626
274.630186	8000.305703	13.175155	-0.054978	4.815629
274.679020	8000.233866	13.180160	-0.054987	4.815608
274.644586	8000.299515	13.185165	-0.054980	4.815627
274.585448	8000.289996	13.190170	-0.054969	4.815625
274.548540	8000.291521	13.195175	-0.054962	4.815625
274.634289	8000.398654	13.200179	-0.054978	4.815656
274.602269	8000.351128	13.205184	-0.054972	4.815642
274.639464	8000.400860	13.210189	-0.054979	4.815657
274.424286	8000.339659	13.215194	-0.054939	4.815640
274.580999	8000.321920	13.220199	-0.054968	4.815634
274.698929	8000.291799	13.225203	-0.054990	4.815625
274.631299	8000.290686	13.230208	-0.054977	4.815625
274.533738	8000.285879	13.235213	-0.054959	4.815624
274.509715	8000.326065	13.240218	-0.054954	4.815636
274.583395	8000.318718	13.245223	-0.054968	4.815633
274.788879	8000.363725	13.250227	-0.055006	4.815645
274.490833	8000.333211	13.255232	-0.054951	4.815638
274.733262	8000.369209	13.260237	-0.054996	4.815647
274.660988	8000.362679	13.265242	-0.054982	4.815646
274.467580	8000.286882	13.270247	-0.054946	4.815624
274.589268	8000.373240	13.275251	-0.054969	4.815649
274.401439	8000.305010	13.280256	-0.054934	4.815630
274.603450	8000.376662	13.285261	-0.054971	4.815650
274.555622	8000.309652	13.290266	-0.054962	4.815631
274.713465	8000.358152	13.295271	-0.054991	4.815644
274.662029	8000.378665	13.300275	-0.054982	4.815650
274.712303	8000.269469	13.305280	-0.054991	4.815618
274.916395	8000.315522	13.310285	-0.055029	4.815631
274.746717	8000.271085	13.315290	-0.054997	4.815618
274.539515	8000.289051	13.320295	-0.054959	4.815625
274.730961	8000.332760	13.325299	-0.054994	4.815636
274.662190	8000.276089	13.330304	-0.054981	4.815620
274.574909	8000.343010	13.335309	-0.054965	4.815640
274.521639	8000.333587	13.340314	-0.054955	4.815638
274.563056	8000.344938	13.345319	-0.054963	4.815641
274.616220	8000.360752	13.350323	-0.054972	4.815645
274.712444	8000.319596	13.355328	-0.054990	4.815633
274.836418	8000.396380	13.360333	-0.055013	4.815655
274.685962	8000.369347	13.365338	-0.054985	4.815647
274.560740	8000.318161	13.370343	-0.054962	4.815633
274.711267	8000.353725	13.375347	-0.054990	4.815643
274.772597	8000.371809	13.380352	-0.055001	4.815648
274.792962	8000.304847	13.385357	-0.055005	4.815628
274.720681	8000.337835	13.390362	-0.054991	4.815638
274.811958	8000.355342	13.395367	-0.055008	4.815643
274.712259	8000.332343	13.400371	-0.054989	4.815636
274.504851	8000.371666	13.405376	-0.054951	4.815649
274.730402	8000.439431	13.410381	-0.054993	4.815668
274.740715	8000.377644	13.415386	-0.054995	4.815650
274.646204	8000.279966	13.420391	-0.054977	4.815621
274.731249	8000.363590	13.425395	-0.054993	4.815646
274.598468	8000.264218	13.430400	-0.054968	4.815617
274.704228	8000.327887	13.435405	-0.054987	4.815635
274.404169	8000.318701	13.440410	-0.054931	4.815634
274.594324	8000.274808	13.445415	-0.054967	4.815620
274.701704	8000.309666	13.450419	-0.054987	4.815630
274.595756	8000.283361	13.455424	-0.054967	4.815623
274.646708	8000.347202	13.460429	-0.054976	4.815641
274.637704	8000.318210	13.465434	-0.054974	4.815633
274.660775	8000.308967	13.470439	-0.054979	4.815630
274.724017	8000.297177	13.475443	-0.054990	4.815626
274.691757	8000.258192	13.480448	-0.054984	4.815615
274.733084	8000.295174	13.485453	-0.054992	4.815626
274.561124	8000.259245	13.490458	-0.054960	4.815616
274.794698	8000.250240	13.495463	-0.055003	4.815612
274.844423	8000.342899	13.500467	-0.055012	4.815639
274.778339	8000.326858	13.505472	-0.055000	4.815635
274.882340	8000.384091	13.510477	-0.055019	4.815651
274.968587	8000.349179	13.515482	-0.055035	4.815640
274.645864	8000.310785	13.520487	-0.054975	4.815631
274.713953	8000.388791	13.525491	-0.054988	4.815653
274.703488	8000.297827	13.530496	-0.054986	4.815626
274.884669	8000.332824	13.535501	-0.055019	4.815636
274.805194	8000.325109	13.540506	-0.055004	4.815634
274.966993	8000.381151	13.545511	-0.055034	4.815650
274.942225	8000.357241	13.550515	-0.055030	4.815643
274.814863	8000.273978	13.555520	-0.055006	4.815619
274.852698	8000.283133	13.560525	-0.055013	4.815621
275.063683	8000.290848	13.565530	-0.055052	4.815623
274.923777	8000.333412	13.570535	-0.055026	4.815636
274.797732	8000.300369	13.575539	-0.055002	4.815627
274.917874	8000.252127	13.580544	-0.055025	4.815612
274.714960	8000.302205	13.585549	-0.054987	4.815628
274.599229	8000.323803	13.590554	-0.054965	4.815635
274.675428	8000.233188	13.595559	-0.054979	4.815608
275.052497	8000.304498	13.600563	-0.055049	4.815627
274.815340	8000.287796	13.605568	-0.055005	4.815623
275.012658	8000.345486	13.610573	-0.055042	4.815639
274.815029	8000.360404	13.615578	-0.055005	4.815644
274.818493	8000.271804	13.620583	-0.055005	4.815618
274.707048	8000.296676	13.625587	-0.054985	4.815626
274.656596	8000.268074	13.630592	-0.054975	4.815618
274.981788	8000.378054	13.635597	-0.055036	4.815649
274.837196	8000.359661	13.640602	-0.055009	4.815644
274.718951	8000.321406	13.645607	-0.054987	4.815633
274.812028	8000.370983	13.650611	-0.055004	4.815647
274.630419	8000.292174	13.655616	-0.054970	4.815625
274.662139	8000.349292	13.660621	-0.054976	4.815642
274.598742	8000.321547	13.665626	-0.054964	4.815634
274.734853	8000.261817	13.670631	-0.054989	4.815616
274.729321	8000.318327	13.675635	-0.054988	4.815632
274.822765	8000.293146	13.680640	-0.055005	4.815625
274.833494	8000.337104	13.685645	-0.055007	4.815637
274.879809	8000.341058	13.690650	-0.055016	4.815638
274.909179	8000.336191	13.695655	-0.055021	4.815637
274.980868	8000.321335	13.700659	-0.055034	4.815632
274.673099	8000.291729	13.705664	-0.054977	4.815625
274.814128	8000.391222	13.710669	-0.055003	4.815653
274.820081	8000.325091	13.715674	-0.055004	4.815634
274.724350	8000.321382	13.720679	-0.054986	4.815633
274.927263	8000.374892	13.725683	-0.055024	4.815648
274.796753	8000.315075	13.730688	-0.055000	4.815631
274.952066	8000.330424	13.735693	-0.055028	4.815635
274.708664	8000.316824	13.740698	-0.054983	4.815632
274.817346	8000.316457	13.745703	-0.055003	4.815631
274.871240	8000.370735	13.750707	-0.055013	4.815647
275.005094	8000.319513	13.755712	-0.055038	4.815631
274.902530	8000.389388	13.760717	-0.055019	4.815652
274.918408	8000.376824	13.765722	-0.055022	4.815649
275.003640	8000.294901	13.770727	-0.055037	4.815624
274.960546	8000.394587	13.775731	-0.055029	4.815654
274.830752	8000.355075	13.780736	-0.055005	4.815643
275.071144	8000.336569	13.785741	-0.055050	4.815636
275.087562	8000.372076	13.790746	-0.055053	4.815646
274.923019	8000.372582	13.795751	-0.055022	4.815647
274.842071	8000.419314	13.800755	-0.055007	4.815661
274.948182	8000.367638	13.805760	-0.055027	4.815646
275.038620	8000.332796	13.810765	-0.055043	4.815635
274.885391	8000.371937	13.815770	-0.055015	4.815647
274.824003	8000.308978	13.820775	-0.055003	4.815629
274.897313	8000.340075	13.825779	-0.055017	4.815638
274.640508	8000.293146	13.830784	-0.054969	4.815626
274.815390	8000.301338	13.835789	-0.055001	4.815627
274.935869	8000.254170	13.840794	-0.055024	4.815613
274.721646	8000.227163	13.845799	-0.054984	4.815606
274.856952	8000.314812	13.850803	-0.055009	4.815631
275.143054	8000.253263	13.855808	-0.055062	4.815611
274.818299	8000.271443	13.860813	-0.055001	4.815618
274.712711	8000.314567	13.865818	-0.054982	4.815631
274.963990	8000.277014	13.870823	-0.055028	4.815619
274.995883	8000.367246	13.875827	-0.055034	4.815646
274.679121	8000.309724	13.880832	-0.054975	4.815630
274.769990	8000.279160	13.885837	-0.054992	4.815621
274.848621	8000.331705	13.890842	-0.055007	4.815636
274.848321	8000.293243	13.895847	-0.055006	4.815625
274.987949	8000.276293	13.900851	-0.055032	4.815619
274.969626	8000.267442	13.905856	-0.055029	4.815616
274.954720	8000.300300	13.910861	-0.055026	4.815626
274.799810	8000.303100	13.915866	-0.054997	4.815628
274.805793	8000.288238	13.920871	-0.054998	4.815623
274.900405	8000.393380	13.925875	-0.055016	4.815654
274.772092	8000.289808	13.930880	-0.054992	4.815624
274.936263	8000.326663	13.935885	-0.055022	4.815634
275.025463	8000.346271	13.940890	-0.055039	4.815639
274.886787	8000.269232	13.945895	-0.055013	4.815617
275.056527	7999.284068	13.950899	-0.055044	4.815329
275.065059	7996.048472	13.955904	-0.055043	4.814383
275.156803	7990.647806	13.960909	-0.055056	4.812803
274.773298	7983.940575	13.965914	-0.054981	4.810843
274.784508	7976.616381	13.970919	-0.054978	4.808699
274.960363	7969.048571	13.975923	-0.055005	4.806482
274.591605	7961.189179	13.980928	-0.054932	4.804182
274.849492	7953.365598	13.985933	-0.054974	4.801888
274.700579	7945.307497	13.990938	-0.054941	4.799526
274.403066	7937.452313	13.995943	-0.054881	4.797223
274.356791	7929.418597	14.000947	-0.054867	4.794865
274.554266	7921.377499	14.005952	-0.054898	4.792503
274.418618	7913.399296	14.010957	-0.054868	4.790159
274.290762	7905.410301	14.015962	-0.054839	4.787812
274.299089	7897.360305	14.020967	-0.054835	4.785444
274.302466	7889.437285	14.025971	-0.054830	4.783113
274.310571	7881.398385	14.030976	-0.054826	4.780747
274.353749	7873.413747	14.035981	-0.054829	4.778395
274.239967	7865.430978	14.040986	-0.054803	4.776043
274.454571	7857.361142	14.045991	-0.054837	4.773663
274.260731	7849.369436	14.050995	-0.054796	4.771307
274.083339	7841.341775	14.056000	-0.054758	4.768938
274.434043	7833.369079	14.061005	-0.054818	4.766583
274.059192	7825.401973	14.066010	-0.054743	4.764231
274.173379	7817.414158	14.071015	-0.054759	4.761870
274.422365	7809.408629	14.076019	-0.054800	4.759502
274.123337	7801.335263	14.081024	-0.054739	4.757114
274.180245	7793.357635	14.086029	-0.054744	4.754753
274.138456	7785.292215	14.091034	-0.054731	4.752364
274.104690	7777.329986	14.096039	-0.054719	4.750005
274.245144	7769.367292	14.101043	-0.054740	4.747645
274.210013	7761.316151	14.106048	-0.054728	4.745257
273.997468	7753.369276	14.111053	-0.054683	4.742899
273.968429	7745.298995	14.116058	-0.054673	4.740504
273.740526	7737.353772	14.121063	-0.054625	4.738144
273.888557	7729.366921	14.126067	-0.054647	4.735770
273.802746	7721.296752	14.131072	-0.054626	4.733371
273.698660	7713.328122	14.136077	-0.054601	4.731001
273.718817	7705.296514	14.141082	-0.054600	4.728610
273.599462	7697.281337	14.146087	-0.054572	4.726224
273.808743	7689.287829	14.151091	-0.054606	4.723842
273.801565	7681.289084	14.156096	-0.054599	4.721457
273.796524	7673.338365	14.161101	-0.054593	4.719086
273.536425	7665.400009	14.166106	-0.054539	4.716718
273.487277	7657.266711	14.171111	-0.054525	4.714290
273.670456	7649.312919	14.176115	-0.054554	4.711914
273.614600	7641.262025	14.181120	-0.054538	4.709508
273.522790	7633.289124	14.186125	-0.054515	4.707125
273.315302	7625.274599	14.191130	-0.054471	4.704728
273.410938	7617.324792	14.196135	-0.054484	4.702348
273.281302	7609.335737	14.201139	-0.054455	4.699956
273.389487	7601.340940	14.206144	-0.054469	4.697560
273.512068	7593.320087	14.211149	-0.054487	4.695156
273.282608	7585.258415	14.216154	-0.054439	4.692739
273.180743	7577.253783	14.221159	-0.054415	4.690337
273.355979	7569.308999	14.226163	-0.054442	4.687951
273.136108	7561.224622	14.231168	-0.054396	4.685523
273.274503	7553.318910	14.236173	-0.054416	4.683147
273.210214	7545.282179	14.241178	-0.054399	4.680731
273.078071	7537.290781	14.246183	-0.054369	4.678327
273.129518	7529.301349	14.251187	-0.054373	4.675922
272.739599	7521.178148	14.256192	-0.054295	4.673476
273.007441	7513.122438	14.261197	-0.054340	4.671048
272.769685	7505.192853	14.266202	-0.054290	4.668658
272.829305	7497.166225	14.271207	-0.054296	4.666237
272.859211	7489.216029	14.276211	-0.054296	4.663838
272.735108	7481.240394	14.281216	-0.054268	4.661430
272.520624	7473.226251	14.286221	-0.054223	4.659009
272.644325	7465.237134	14.291226	-0.054241	4.656594
272.516504	7457.200744	14.296231	-0.054211	4.654164
272.812268	7449.251378	14.301235	-0.054261	4.651758
272.611183	7441.196360	14.306240	-0.054218	4.649320
272.626333	7433.248240	14.311245	-0.054216	4.646913
272.619192	7425.223852	14.316250	-0.054209	4.644481
272.413732	7417.236174	14.321255	-0.054166	4.642059
272.457795	7409.223426	14.326259	-0.054169	4.639629
272.433315	7401.235309	14.331264	-0.054159	4.637204
272.267200	7393.196680	14.336269	-0.054123	4.634763
272.339423	7385.177089	14.341274	-0.054131	4.632326
272.364185	7377.147265	14.346279	-0.054130	4.629885
272.288021	7369.202632	14.351283	-0.054111	4.627469
272.334393	7361.158708	14.356288	-0.054114	4.625021
272.545014	7353.268809	14.361293	-0.054148	4.622618
272.488661	7345.195314	14.366298	-0.054132	4.620159
272.331572	7337.197798	14.371303	-0.054098	4.617721
272.425306	7329.185156	14.376307	-0.054110	4.615278
272.213224	7321.135840	14.381312	-0.054065	4.612821
271.944043	7313.150215	14.386317	-0.054009	4.610384
272.063766	7305.174873	14.391322	-0.054026	4.607947
272.040608	7297.115978	14.396327	-0.054017	4.605484
272.029842	7289.199197	14.401331	-0.054010	4.603064
271.903357	7281.147972	14.406336	-0.053981	4.600600
272.081264	7273.210857	14.411341	-0.054009	4.598171
271.893922	7265.159169	14.416346	-0.053968	4.595705
272.002674	7257.152141	14.421351	-0.053983	4.593251
271.985649	7249.092581	14.426355	-0.053975	4.590780
271.876406	7241.107766	14.431360	-0.053949	4.588331
271.756566	7233.141526	14.436365	-0.053922	4.585885
271.650103	7225.140936	14.441370	-0.053896	4.583428
271.602909	7217.107963	14.446375	-0.053882	4.580960
271.491178	7209.152625	14.451379	-0.053856	4.578514
271.506950	7201.146414	14.456384	-0.053854	4.576052
271.558568	7193.123104	14.461389	-0.053858	4.573583
271.736788	7185.059089	14.466394	-0.053886	4.571100
271.335151	7177.102773	14.471399	-0.053806	4.568648
271.425094	7169.132839	14.476403	-0.053817	4.566191
271.445104	7161.105716	14.481408	-0.053816	4.563715
271.299810	7153.151401	14.486413	-0.053784	4.561261
271.154392	7145.180205	14.491418	-0.053751	4.558799
271.363892	7137.161252	14.496423	-0.053785	4.556322
271.262038	7129.123827	14.501427	-0.053761	4.553838
271.376548	7121.058484	14.506432	-0.053777	4.551344
271.272419	7113.057148	14.511437	-0.053752	4.548868
271.102255	7105.104926	14.516442	-0.053715	4.546405
271.135629	7097.099542	14.521447	-0.053716	4.543925
271.306420	7089.152119	14.526451	-0.053742	4.541462
271.153322	7081.092096	14.531456	-0.053709	4.538963
270.975374	7073.148389	14.536461	-0.053670	4.536498
270.780501	7065.122723	14.541466	-0.053629	4.534006
270.938241	7057.079174	14.546471	-0.053653	4.531507
271.066235	7049.143644	14.551475	-0.053671	4.529041
270.902830	7041.109006	14.556480	-0.053635	4.526542
271.052961	7033.128828	14.561485	-0.053658	4.524060
270.931041	7025.142922	14.566490	-0.053630	4.521573
270.798671	7017.111441	14.571495	-0.053600	4.519071
270.627040	7009.136844	14.576499	-0.053563	4.516586
270.648730	7001.094135	14.581504	-0.053562	4.514078
270.729907	6993.016403	14.586509	-0.053571	4.511558
270.707724	6985.052989	14.591514	-0.053562	4.509072
270.631951	6977.056464	14.596519	-0.053543	4.506574
270.678804	6969.077337	14.601523	-0.053546	4.504080
270.604505	6961.063759	14.606528	-0.053527	4.501574
270.562798	6953.072345	14.611533	-0.053514	4.499074
270.373356	6945.096726	14.616538	-0.053473	4.496577
270.412830	6937.047741	14.621543	-0.053475	4.494055
270.369636	6929.061820	14.626547	-0.053462	4.491553
270.570380	6921.007323	14.631552	-0.053494	4.489028
270.461085	6913.044933	14.636557	-0.053468	4.486529
270.274655	6905.076877	14.641562	-0.053428	4.484027
270.248468	6897.074926	14.646567	-0.053418	4.481513
270.505929	6889.118189	14.651571	-0.053461	4.479014
270.168262	6881.088816	14.656576	-0.053393	4.476488
270.306837	6873.071807	14.661581	-0.053413	4.473966
270.323597	6865.015022	14.666586	-0.053411	4.471429
270.114038	6857.015907	14.671591	-0.053367	4.468909
269.985596	6849.022441	14.676595	-0.053337	4.466389
270.195852	6841.019683	14.681600	-0.053371	4.463866
270.246609	6833.010413	14.686605	-0.053375	4.461339
270.134446	6825.021481	14.691610	-0.053349	4.458817
270.023585	6817.027226	14.696615	-0.053323	4.456291
270.051139	6809.060515	14.701619	-0.053323	4.453773
269.875935	6801.014026	14.706624	-0.053285	4.451228
269.940319	6793.018453	14.711629	-0.053292	4.448698
269.853634	6785.033327	14.716634	-0.053270	4.446170
269.922349	6776.990627	14.721639	-0.053278	4.443622
269.876653	6769.076159	14.726643	-0.053264	4.441113
269.714273	6761.003434	14.731648	-0.053229	4.438552
269.752718	6753.016263	14.736653	-0.053230	4.436018
269.692937	6744.978999	14.741658	-0.053214	4.433466
269.585241	6736.949041	14.746663	-0.053189	4.430914
269.662808	6728.981963	14.751667	-0.053198	4.428382
269.534443	6720.943926	14.756672	-0.053169	4.425824
269.542705	6712.994874	14.761677	-0.053165	4.423295
269.618457	6704.977811	14.766682	-0.053174	4.420742
269.519380	6696.969973	14.771687	-0.053150	4.418190
269.279619	6689.007154	14.776691	-0.053100	4.415650
269.166077	6680.985412	14.781696	-0.053073	4.413091
269.332243	6672.974721	14.786701	-0.053099	4.410535
269.258892	6665.004692	14.791706	-0.053080	4.407989
269.229859	6656.947752	14.796711	-0.053069	4.405415
269.299395	6649.007164	14.801715	-0.053077	4.402876
269.399072	6640.958445	14.806720	-0.053090	4.400302
269.078792	6633.028688	14.811725	-0.053025	4.397762
269.233599	6625.014721	14.816730	-0.053049	4.395196
269.089428	6616.949149	14.821735	-0.053017	4.392610
269.192349	6608.968788	14.826739	-0.053031	4.390052
268.959938	6600.949311	14.831744	-0.052982	4.387477
268.944442	6592.961910	14.836749	-0.052974	4.384913
268.939117	6585.010104	14.841754	-0.052968	4.382358
268.811045	6576.963209	14.846759	-0.052938	4.379771
269.031241	6569.032182	14.851763	-0.052974	4.377222
268.848232	6560.977366	14.856768	-0.052935	4.374629
268.656009	6552.995430	14.861773	-0.052894	4.372057
268.707541	6544.981707	14.866778	-0.052898	4.369476
268.661020	6536.973608	14.871783	-0.052884	4.366894
268.741874	6529.018134	14.876787	-0.052894	4.364328
268.800736	6521.013589	14.881792	-0.052900	4.361745
268.836147	6512.972675	14.886797	-0.052901	4.359148
268.780130	6505.042672	14.891802	-0.052885	4.356586
268.620386	6496.972721	14.896807	-0.052850	4.353975
268.578749	6488.901433	14.901811	-0.052837	4.351364
268.403269	6480.918736	14.906816	-0.052799	4.348778
268.268472	6472.937134	14.911821	-0.052769	4.346192
268.315919	6464.960405	14.916826	-0.052772	4.343607
268.331606	6456.970796	14.921831	-0.052770	4.341016
268.267415	6448.988613	14.926835	-0.052753	4.338426
268.183251	6440.949178	14.931840	-0.052732	4.335815
268.407293	6432.952166	14.936845	-0.052768	4.333218
268.223078	6424.935154	14.941850	-0.052728	4.330611
268.257601	6416.938396	14.946855	-0.052729	4.328010
268.317982	6408.964086	14.951859	-0.052735	4.325415
268.126074	6400.929268	14.956864	-0.052694	4.322796
268.035047	6392.949805	14.961869	-0.052672	4.320196
268.133848	6385.001504	14.966874	-0.052685	4.317605
268.109920	6376.967967	14.971879	-0.052675	4.314983
268.069818	6368.952132	14.976883	-0.052663	4.312366
267.942665	6360.882070	14.981888	-0.052634	4.309729
268.188129	6352.879857	14.986893	-0.052674	4.307115
268.119634	6344.922301	14.991898	-0.052656	4.304512
267.846364	6336.929666	14.996903	-0.052600	4.301894
267.960179	6328.950794	15.001907	-0.052616	4.299282
267.852189	6320.944973	15.006912	-0.052590	4.296658
267.783210	6312.938380	15.011917	-0.052572	4.294033
267.604850	6304.932759	15.016922	-0.052534	4.291405
267.852213	6296.859732	15.021927	-0.052574	4.288757
267.811727	6288.938493	15.026931	-0.052562	4.286155
267.569163	6280.953124	15.031936	-0.052511	4.283528
267.632106	6272.920378	15.036941	-0.052518	4.280887
267.553985	6264.988188	15.041946	-0.052498	4.278276
267.407270	6256.938483	15.046951	-0.052465	4.275624
267.591436	6248.934483	15.051955	-0.052494	4.272989
267.492301	6240.861372	15.056960	-0.052470	4.270326
267.608898	6232.918204	15.061965	-0.052487	4.267707
267.289699	6224.889357	15.066970	-0.052422	4.265054
267.344901	6216.927419	15.071975	-0.052427	4.262424
267.388793	6208.888529	15.076979	-0.052430	4.259768
267.338948	6200.924198	15.081984	-0.052415	4.257134
267.288725	6192.888441	15.086989	-0.052401	4.254474
267.039903	6184.916941	15.091994	-0.052349	4.251832
266.981997	6176.867960	15.096999	-0.052333	4.249165
267.125117	6168.952115	15.102003	-0.052354	4.246542
267.095882	6160.930250	15.107008	-0.052344	4.243880
267.027449	6152.924890	15.112013	-0.052326	4.241222
266.866109	6144.966701	15.117018	-0.052290	4.238577
266.618614	6136.938091	15.122023	-0.052239	4.235906
266.937228	6128.927361	15.127027	-0.052293	4.233245
266.959682	6120.868279	15.132032	-0.052292	4.230563
266.994317	6112.891739	15.137037	-0.052293	4.227907
266.901765	6104.921149	15.142042	-0.052270	4.225250
266.931239	6096.937016	15.147047	-0.052271	4.222589
266.971504	6088.946365	15.152051	-0.052273	4.219923
266.785128	6080.940465	15.157056	-0.052233	4.217248
266.454999	6072.973044	15.162061	-0.052166	4.214583
266.477769	6064.905746	15.167066	-0.052165	4.211887
266.686430	6056.909755	15.172071	-0.052198	4.209215
266.572930	6048.958552	15.177075	-0.052172	4.206552
266.450136	6040.953084	15.182080	-0.052144	4.203870
266.446919	6032.982573	15.187085	-0.052138	4.201199
266.492376	6024.953252	15.192090	-0.052141	4.198506
266.420152	6016.945816	15.197095	-0.052122	4.195819
266.412792	6008.864336	15.202099	-0.052116	4.193105
266.418340	6000.792329	15.207104	-0.052111	4.190393
266.471908	5992.855822	15.212109	-0.052116	4.187725
266.423541	5984.903544	15.217114	-0.052102	4.185049
266.266615	5976.926544	15.222119	-0.052067	4.182362
266.238264	5968.914391	15.227123	-0.052057	4.179663
266.005517	5960.930845	15.232128	-0.052008	4.176969
266.174864	5952.916996	15.237133	-0.052034	4.174268
266.179118	5944.862928	15.242138	-0.052030	4.171550
266.017106	5936.887158	15.247143	-0.051994	4.168854
266.187887	5928.912768	15.252147	-0.052021	4.166161
266.100328	5920.915332	15.257152	-0.051999	4.163456
265.979336	5912.903990	15.262157	-0.051971	4.160743
265.829135	5904.981884	15.267162	-0.051938	4.158059
265.820060	5896.888766	15.272167	-0.051931	4.155317
265.682342	5888.888314	15.277171	-0.051900	4.152602
265.591528	5880.832647	15.282176	-0.051878	4.149868
265.713821	5872.849307	15.287181	-0.051895	4.147159
265.660865	5864.868146	15.292186	-0.051880	4.144447
265.698344	5856.924830	15.297191	-0.051882	4.141747
265.734312	5848.889490	15.302195	-0.051883	4.139014
265.686582	5840.897295	15.307200	-0.051869	4.136293
265.527174	5832.896094	15.312205	-0.051834	4.133566
265.531914	5824.853086	15.317210	-0.051830	4.130824
265.398631	5816.857975	15.322215	-0.051800	4.128096
265.436036	5808.898529	15.327219	-0.051801	4.125379
265.382306	5800.906555	15.332224	-0.051786	4.122649
265.140799	5792.888512	15.337229	-0.051736	4.119906
265.394035	5784.948741	15.342234	-0.051778	4.117194
265.426524	5776.889222	15.347239	-0.051778	4.114436
265.448322	5768.852819	15.352243	-0.051777	4.111684
265.441005	5760.856595	15.357248	-0.051770	4.108944
265.374356	5752.857961	15.362253	-0.051753	4.106201
265.185866	5744.902110	15.367258	-0.051712	4.103468
264.963920	5736.879305	15.372263	-0.051666	4.100711
265.158406	5728.928572	15.377267	-0.051697	4.097981
265.046768	5720.886925	15.382272	-0.051671	4.095215
264.843396	5712.901513	15.387277	-0.051627	4.092465
265.064044	5704.871400	15.392282	-0.051663	4.089703
265.033959	5696.912669	15.397287	-0.051652	4.086961
264.814632	5688.912475	15.402291	-0.051606	4.084200
264.932924	5680.956829	15.407296	-0.051623	4.081457
264.920859	5672.932144	15.412301	-0.051615	4.078686
264.825821	5664.983111	15.417306	-0.051592	4.075939
264.798383	5656.912168	15.422311	-0.051582	4.073148
264.878073	5648.907388	15.427315	-0.051592	4.070380
264.828531	5640.901573	15.432320	-0.051577	4.067608
264.568323	5632.904462	15.437325	-0.051523	4.064834
264.657664	5624.957071	15.442330	-0.051535	4.062081
264.545815	5616.930680	15.447335	-0.051508	4.059295
264.679714	5608.969781	15.452339	-0.051528	4.056534
264.736205	5600.924040	15.457344	-0.051533	4.053740
264.715062	5592.925692	15.462349	-0.051524	4.050959
264.418214	5584.955225	15.467354	-0.051464	4.048183
264.374671	5576.919570	15.472359	-0.051450	4.045385
264.532424	5568.947253	15.477363	-0.051474	4.042610
264.338181	5560.943440	15.482368	-0.051433	4.039818
264.263597	5552.996491	15.487373	-0.051414	4.037045
264.318288	5544.926080	15.492378	-0.051418	4.034229
264.235316	5536.808271	15.497383	-0.051398	4.031392
264.211630	5528.892758	15.502387	-0.051388	4.028625
264.099091	5520.883966	15.507392	-0.051362	4.025822
264.056327	5512.925005	15.512397	-0.051348	4.023036
263.926166	5504.921079	15.517402	-0.051319	4.020230
263.859610	5496.933344	15.522407	-0.051301	4.017430
263.956666	5488.929710	15.527411	-0.051314	4.014624
263.844712	5480.888503	15.532416	-0.051288	4.011800
263.746137	5472.879957	15.537421	-0.051264	4.008985
263.848698	5464.942617	15.542426	-0.051278	4.006197
263.944141	5456.935670	15.547431	-0.051290	4.003382
263.815222	5448.943617	15.552435	-0.051261	4.000567
263.860099	5440.937811	15.557440	-0.051264	3.997748
263.821126	5432.936167	15.562445	-0.051252	3.994927
263.727599	5424.922356	15.567450	-0.051229	3.992099
263.513255	5416.890672	15.572455	-0.051184	3.989260
263.487278	5408.940887	15.577459	-0.051174	3.986452
263.462872	5400.939261	15.582464	-0.051164	3.983623
263.566595	5392.917055	15.587469	-0.051178	3.980787
263.378915	5384.991792	15.592474	-0.051138	3.977978
263.297314	5376.923607	15.597479	-0.051117	3.975119
263.394814	5368.935549	15.602483	-0.051130	3.972289
263.264598	5360.932300	15.607488	-0.051100	3.969447
263.321543	5352.951408	15.612493	-0.051106	3.966615
263.250468	5344.967397	15.617498	-0.051087	3.963777
263.041842	5336.986101	15.622503	-0.051043	3.960936
263.303142	5329.010741	15.627507	-0.051086	3.958103
263.288685	5320.995625	15.632512	-0.051078	3.955250
263.221429	5312.931065	15.637517	-0.051061	3.952375
263.231899	5304.950014	15.642522	-0.051057	3.949530
263.161536	5296.949818	15.647527	-0.051039	3.946674
263.117712	5288.956764	15.652531	-0.051025	3.943819
263.071279	5280.975767	15.657536	-0.051011	3.940967
263.025669	5272.991806	15.662541	-0.050998	3.938111
263.107150	5265.014306	15.667546	-0.051007	3.935258
262.784855	5256.979101	15.672551	-0.050942	3.932375
262.924428	5248.976375	15.677555	-0.050963	3.929509
262.921271	5241.004035	15.682560	-0.050957	3.926650
262.858198	5232.986627	15.687565	-0.050940	3.923772
262.871777	5225.038152	15.692570	-0.050937	3.920917
262.816918	5217.024281	15.697575	-0.050922	3.918036
262.660069	5208.995527	15.702579	-0.050887	3.915145
262.495945	5200.987022	15.707584	-0.050851	3.912260
262.607898	5192.971130	15.712589	-0.050867	3.909374
262.665186	5185.004635	15.717594	-0.050872	3.906504
262.557062	5176.969524	15.722599	-0.050847	3.903603
262.601572	5168.986074	15.727603	-0.050850	3.900722
262.652803	5161.021117	15.732608	-0.050854	3.897845
262.531999	5153.015820	15.737613	-0.050826	3.894948
262.440984	5144.980464	15.742618	-0.050804	3.892039
262.308393	5136.967153	15.747623	-0.050774	3.889135
262.348281	5128.986900	15.752627	-0.050776	3.886244
262.229392	5121.018460	15.757632	-0.050749	3.883352
262.241433	5112.985369	15.762637	-0.050746	3.880437
262.294378	5105.069550	15.767642	-0.050750	3.877564
262.267071	5096.998184	15.772647	-0.050740	3.874630
262.120296	5088.763522	15.777651	-0.050707	3.871631
262.057690	5080.829954	15.782656	-0.050690	3.868742
261.964991	5072.863719	15.787661	-0.050668	3.865839
261.984152	5064.974447	15.792666	-0.050666	3.862963
262.155099	5056.922755	15.797671	-0.050692	3.860029
262.242516	5049.015918	15.802675	-0.050703	3.857144
261.874737	5041.026517	15.807680	-0.050630	3.854217
261.928263	5032.974754	15.812685	-0.050634	3.851274
262.009089	5024.989867	15.817690	-0.050644	3.848354
261.897233	5016.995355	15.822695	-0.050618	3.845424
261.903256	5009.027635	15.827699	-0.050614	3.842504
261.752562	5001.006717	15.832704	-0.050580	3.839559
261.669033	4993.055402	15.837709	-0.050560	3.836638
261.591379	4985.064824	15.842714	-0.050540	3.833702
261.681167	4976.997043	15.847719	-0.050551	3.830738
261.614671	4969.044477	15.852723	-0.050534	3.827810
261.560300	4961.026136	15.857728	-0.050518	3.824857
261.395223	4953.072883	15.862733	-0.050482	3.821923
261.578369	4945.060911	15.867738	-0.050511	3.818972
261.618296	4937.084474	15.872743	-0.050513	3.816030
261.559684	4929.080177	15.877747	-0.050497	3.813072
261.449485	4921.069080	15.882752	-0.050471	3.810109
261.444797	4913.077518	15.887757	-0.050465	3.807152
261.407574	4905.099977	15.892762	-0.050453	3.804198
261.267702	4897.108572	15.897767	-0.050421	3.801235
261.324931	4889.151411	15.902771	-0.050427	3.798286
261.176206	4881.121756	15.907776	-0.050394	3.795303
261.186383	4873.067210	15.912781	-0.050390	3.792312
261.251629	4865.042614	15.917786	-0.050397	3.789331
261.061030	4857.075664	15.922791	-0.050356	3.786364
260.902399	4849.084630	15.927795	-0.050321	3.783386
260.947896	4841.103614	15.932800	-0.050325	3.780413
260.840478	4833.121338	15.937805	-0.050299	3.777435
260.829264	4825.130392	15.942810	-0.050292	3.774453
260.810116	4817.078559	15.947815	-0.050283	3.771446
260.918554	4809.086358	15.952819	-0.050298	3.768462
260.802715	4801.114975	15.957824	-0.050271	3.765478
260.867284	4793.096397	15.962829	-0.050278	3.762478
260.828903	4785.120510	15.967834	-0.050265	3.759489
260.802046	4777.122808	15.972839	-0.050255	3.756490
260.683162	4769.123062	15.977843	-0.050228	3.753486
260.798600	4761.077015	15.982848	-0.050244	3.750467
260.741102	4753.091344	15.987853	-0.050228	3.747465
260.647681	4745.114347	15.992858	-0.050205	3.744462
260.320431	4737.147655	15.997863	-0.050139	3.741456
260.444494	4729.160004	16.002867	-0.050157	3.738450
260.308749	4721.171918	16.007872	-0.050126	3.735435
260.189154	4713.120682	16.012877	-0.050099	3.732394
260.225022	4705.129018	16.017882	-0.050100	3.729377
260.092673	4697.158634	16.022887	-0.050070	3.726361
260.042854	4689.187029	16.027891	-0.050056	3.723345
260.201075	4681.170685	16.032896	-0.050080	3.720314
260.231859	4673.209348	16.037901	-0.050080	3.717298
260.341574	4665.189304	16.042906	-0.050095	3.714260
260.039353	4657.062567	16.047911	-0.050034	3.711169
260.171528	4649.137293	16.052915	-0.050053	3.708162
260.020019	4641.147324	16.057920	-0.050019	3.705121
259.959913	4633.158036	16.062925	-0.050003	3.702080
259.982662	4625.209277	16.067930	-0.050002	3.699054
259.789086	4617.224679	16.072935	-0.049961	3.696007
259.681415	4609.217383	16.077939	-0.049935	3.692950
259.670605	4601.185860	16.082944	-0.049928	3.689885
259.807902	4593.196983	16.087949	-0.049948	3.686836
259.603493	4585.260979	16.092954	-0.049905	3.683797
259.512217	4577.232756	16.097959	-0.049883	3.680723
259.755195	4569.267233	16.102963	-0.049923	3.677679
259.771769	4561.226449	16.107968	-0.049920	3.674597
259.737866	4553.190913	16.112973	-0.049909	3.671514
259.677700	4545.233820	16.117978	-0.049892	3.668457
259.497556	4537.228944	16.122983	-0.049853	3.665377
259.428127	4529.276143	16.127987	-0.049835	3.662317
259.511170	4521.249145	16.132992	-0.049845	3.659229
259.500746	4513.257121	16.137997	-0.049838	3.656151
259.543925	4505.242282	16.143002	-0.049841	3.653062
259.190873	4497.229773	16.148007	-0.049770	3.649961
259.261352	4489.274371	16.153011	-0.049778	3.646890
259.192717	4481.259322	16.158016	-0.049760	3.643790
259.223863	4473.269253	16.163021	-0.049760	3.640700
259.339061	4465.329312	16.168026	-0.049776	3.637629
259.340732	4457.279888	16.173031	-0.049771	3.634510
259.001220	4449.290886	16.178035	-0.049703	3.631402
258.818741	4441.279435	16.183040	-0.049663	3.628287
258.779868	4433.256873	16.188045	-0.049651	3.625169
258.929177	4425.301870	16.193050	-0.049673	3.622080
258.752558	4417.330011	16.198055	-0.049635	3.618973
258.892985	4409.337915	16.203059	-0.049656	3.615864
258.864043	4401.322190	16.208064	-0.049645	3.612738
258.698388	4393.271932	16.213069	-0.049609	3.609592
258.796019	4385.343494	16.218074	-0.049622	3.606498
258.740212	4377.338553	16.223079	-0.049606	3.603368
258.591961	4369.375925	16.228083	-0.049574	3.600249
258.580936	4361.398478	16.233088	-0.049566	3.597125
258.644645	4353.341375	16.238093	-0.049573	3.593969
258.671831	4345.344878	16.243098	-0.049573	3.590834
258.405543	4337.371006	16.248103	-0.049518	3.587696
258.516499	4329.370544	16.253107	-0.049533	3.584555
258.317343	4321.445605	16.258112	-0.049491	3.581433
258.130563	4313.405471	16.263117	-0.049451	3.578263
258.452221	4305.423337	16.268122	-0.049505	3.575127
258.358255	4297.385119	16.273127	-0.049482	3.571955
258.248364	4289.405865	16.278131	-0.049457	3.568803
258.232154	4281.427609	16.283136	-0.049448	3.565651
258.412004	4273.414322	16.288141	-0.049477	3.562488
258.602970	4265.436433	16.293146	-0.049507	3.559337
258.297686	4257.481078	16.298151	-0.049445	3.556177
258.066179	4249.390476	16.303155	-0.049396	3.552963
258.281072	4241.320411	16.308160	-0.049431	3.549767
257.978640	4233.381075	16.313165	-0.049369	3.546605
257.894623	4225.412172	16.318170	-0.049348	3.543435
257.848274	4217.414670	16.323175	-0.049334	3.540252
257.797169	4209.443553	16.328179	-0.049320	3.537076
257.751405	4201.451035	16.333184	-0.049306	3.533889
257.701505	4193.412873	16.338189	-0.049291	3.530681
257.788385	4185.449811	16.343194	-0.049302	3.527504
257.585277	4177.433982	16.348199	-0.049259	3.524294
257.568347	4169.489353	16.353203	-0.049251	3.521116
257.672817	4161.500533	16.358208	-0.049265	3.517920
257.516174	4153.495354	16.363213	-0.049230	3.514708
257.570614	4145.496897	16.368218	-0.049235	3.511501
257.519094	4137.479698	16.373223	-0.049220	3.508281
257.378076	4129.493891	16.378227	-0.049189	3.505067
257.354022	4121.518827	16.383232	-0.049179	3.501859
257.378841	4113.547292	16.388237	-0.049178	3.498650
257.477616	4105.554071	16.393242	-0.049191	3.495432
257.343985	4097.523647	16.398247	-0.049161	3.492189
257.208233	4089.552704	16.403251	-0.049131	3.488967
257.399897	4081.569682	16.408256	-0.049161	3.485747
257.134686	4073.587453	16.413261	-0.049106	3.482510
257.301795	4065.621852	16.418266	-0.049132	3.479291
257.280531	4057.635315	16.423271	-0.049123	3.476054
257.423542	4049.570894	16.428275	-0.049144	3.472788
257.155389	4041.553574	16.433280	-0.049089	3.469524
256.892947	4033.581101	16.438285	-0.049035	3.466276
257.105679	4025.612060	16.443290	-0.049069	3.463042
257.021165	4017.612832	16.448295	-0.049048	3.459782
256.794394	4009.650974	16.453299	-0.049001	3.456531
256.837008	4001.640635	16.458304	-0.049003	3.453265
256.851732	3993.611827	16.463309	-0.049001	3.449987
257.068420	3985.649930	16.468314	-0.049036	3.446741
256.917087	3977.639795	16.473319	-0.049002	3.443459
256.696588	3969.674996	16.478323	-0.048956	3.440191
256.585762	3961.715803	16.483328	-0.048930	3.436925
256.659633	3953.667015	16.488333	-0.048938	3.433626
256.802575	3945.644606	16.493338	-0.048960	3.430336
256.644496	3937.660570	16.498343	-0.048925	3.427050
256.592805	3929.692220	16.503347	-0.048910	3.423770
256.656916	3921.707606	16.508352	-0.048917	3.420484
256.614659	3913.723518	16.513357	-0.048904	3.417191
256.483944	3905.743121	16.518362	-0.048874	3.413894
256.215812	3897.704825	16.523367	-0.048819	3.410565
256.293431	3889.737865	16.528371	-0.048828	3.407274
256.405117	3881.716160	16.533376	-0.048843	3.403959
256.204386	3873.769741	16.538381	-0.048801	3.400660
256.416990	3865.799554	16.543386	-0.048835	3.397363
256.235866	3857.782810	16.548391	-0.048796	3.394030
256.063480	3849.731985	16.553395	-0.048759	3.390679
256.003164	3841.750300	16.558400	-0.048742	3.387358
255.872628	3833.763664	16.563405	-0.048712	3.384029
255.850073	3825.817004	16.568410	-0.048703	3.380717
256.030826	3817.807777	16.573415	-0.048731	3.377383
255.992253	3809.826522	16.578419	-0.048719	3.374050
255.596277	3801.832113	16.583424	-0.048640	3.370695
255.541322	3793.838360	16.588429	-0.048624	3.367349
255.851373	3785.841455	16.593434	-0.048677	3.364012
255.723960	3777.860845	16.598439	-0.048648	3.360662
255.593256	3769.907133	16.603443	-0.048618	3.357320
255.528583	3761.882902	16.608448	-0.048601	3.353948
255.824576	3753.815582	16.613453	-0.048651	3.350567
255.647678	3745.878774	16.618458	-0.048612	3.347221
255.412490	3737.874306	16.623463	-0.048563	3.343840
255.491260	3729.900328	16.628467	-0.048573	3.340480
255.395060	3721.946631	16.633472	-0.048550	3.337120
255.262692	3713.936951	16.638477	-0.048520	3.333730
255.369999	3705.946227	16.643482	-0.048534	3.330355
255.331895	3697.935780	16.648487	-0.048522	3.326962
255.218741	3689.975467	16.653491	-0.048495	3.323584
255.119718	3682.019854	16.658496	-0.048472	3.320205
255.214110	3673.991386	16.663501	-0.048484	3.316798
255.281040	3665.994841	16.668506	-0.048491	3.313401
255.099860	3657.963953	16.673511	-0.048452	3.309977
255.167364	3649.997735	16.678515	-0.048459	3.306586
255.016043	3642.013788	16.683520	-0.048426	3.303175
254.802727	3634.032735	16.688525	-0.048381	3.299760
255.067918	3626.075654	16.693530	-0.048425	3.296370
254.933977	3618.021641	16.698535	-0.048395	3.292920
254.858212	3610.045236	16.703539	-0.048375	3.289501
254.938485	3602.076215	16.708544	-0.048385	3.286088
254.824076	3594.085014	16.713549	-0.048358	3.282654
254.902995	3586.121070	16.718554	-0.048368	3.279236
254.695874	3578.144152	16.723559	-0.048324	3.275798
254.921739	3570.082747	16.728563	-0.048361	3.272337
254.939594	3562.110248	16.733568	-0.048359	3.268902
254.657314	3554.117079	16.738573	-0.048301	3.265443
254.502173	3546.176537	16.743578	-0.048267	3.262008
254.783702	3538.147418	16.748583	-0.048314	3.258548
254.679367	3530.175092	16.753587	-0.048289	3.255094
254.530665	3522.176468	16.758592	-0.048256	3.251623
254.455503	3514.162414	16.763597	-0.048237	3.248144
254.384650	3506.197556	16.768602	-0.048218	3.244683
254.238352	3498.223088	16.773607	-0.048186	3.241212
254.604050	3490.218355	16.778611	-0.048249	3.237744
254.571496	3482.254027	16.783616	-0.048237	3.234274
254.200409	3474.184520	16.788621	-0.048163	3.230740
254.254181	3466.219482	16.793626	-0.048168	3.227266
254.197359	3458.227641	16.798631	-0.048152	3.223771
253.956682	3450.271714	16.803635	-0.048102	3.220281
253.970621	3442.302759	16.808640	-0.048099	3.216792
254.021453	3434.287016	16.813645	-0.048103	3.213280
254.007227	3426.288283	16.818650	-0.048095	3.209769
253.785629	3418.300864	16.823655	-0.048049	3.206251
253.783994	3410.342643	16.828659	-0.048043	3.202750
254.022096	3402.355499	16.833664	-0.048082	3.199243
253.788838	3394.375802	16.838669	-0.048033	3.195716
253.593911	3386.387948	16.843674	-0.047992	3.192183
253.778668	3378.350190	16.848679	-0.048021	3.188640
253.611959	3370.369008	16.853683	-0.047985	3.185103
253.586879	3362.409982	16.858688	-0.047975	3.181578
253.445353	3354.442114	16.863693	-0.047943	3.178040
253.572058	3346.440504	16.868698	-0.047961	3.174494
253.386989	3338.427968	16.873703	-0.047922	3.170927
253.502315	3330.429197	16.878707	-0.047938	3.167374
253.513065	3322.435455	16.883712	-0.047934	3.163816
253.278707	3314.485681	16.888717	-0.047886	3.160262
253.195014	3306.551300	16.893722	-0.047865	3.156717
253.174922	3298.499555	16.898727	-0.047856	3.153119
253.116667	3290.483061	16.903731	-0.047839	3.149531
253.005580	3282.501108	16.908736	-0.047814	3.145952
253.079754	3274.508059	16.913741	-0.047822	3.142372
253.258396	3266.525649	16.918746	-0.047850	3.138797
253.171890	3258.556799	16.923751	-0.047829	3.135213
252.905923	3250.580805	16.928755	-0.047774	3.131613
252.973020	3242.588851	16.933760	-0.047781	3.128017
252.866116	3234.564450	16.938765	-0.047756	3.124394
253.019560	3226.648027	16.943770	-0.047779	3.120828
253.009194	3218.639474	16.948775	-0.047772	3.117208
252.970019	3210.643098	16.953779	-0.047759	3.113589
252.861008	3202.651986	16.958784	-0.047734	3.109964
252.663859	3194.670108	16.963789	-0.047692	3.106335
252.802342	3186.686742	16.968794	-0.047712	3.102717
252.697815	3178.694436	16.973799	-0.047687	3.099079
252.676630	3170.715536	16.978803	-0.047678	3.095447
252.875367	3162.702645	16.983808	-0.047710	3.091805
252.790648	3154.709905	16.988813	-0.047689	3.088155
252.609934	3146.763005	16.993818	-0.047650	3.084517
252.646212	3138.803604	16.998823	-0.047651	3.080880
252.681535	3130.817561	17.003827	-0.047653	3.077225
252.567902	3122.807114	17.008832	-0.047626	3.073549
252.324826	3114.750821	17.013837	-0.047576	3.069840
252.411552	3106.771929	17.018842	-0.047587	3.066178
252.386540	3098.793600	17.023847	-0.047577	3.062507
252.331761	3090.839418	17.028851	-0.047561	3.058841
252.258195	3082.908233	17.033856	-0.047542	3.055181
252.148520	3074.867299	17.038861	-0.047516	3.051464
252.048382	3066.885867	17.043866	-0.047492	3.047770
252.096093	3058.908349	17.048871	-0.047496	3.044080
251.939855	3050.959543	17.053875	-0.047462	3.040389
252.056318	3042.980122	17.058880	-0.047478	3.036693
252.075968	3034.943824	17.063885	-0.047476	3.032962
252.180827	3026.948807	17.068890	-0.047491	3.029249
251.857743	3018.996717	17.073895	-0.047425	3.025530
251.701412	3011.037172	17.078899	-0.047391	3.021812
251.722330	3003.057615	17.083904	-0.047389	3.018088
251.627786	2995.057262	17.088909	-0.047367	3.014345
251.724047	2987.056214	17.093914	-0.047379	3.010606
251.558285	2979.073953	17.098919	-0.047343	3.006858
251.768796	2971.088049	17.103923	-0.047377	3.003122
251.794062	2963.108933	17.108928	-0.047376	2.999375
251.524381	2955.153697	17.113933	-0.047321	2.995621
251.686724	2947.135002	17.118938	-0.047346	2.991853
251.636119	2939.125752	17.123943	-0.047331	2.988075
251.342544	2931.170987	17.128947	-0.047271	2.984305
251.504837	2923.196379	17.133952	-0.047296	2.980544
251.482704	2915.203956	17.138957	-0.047287	2.976760
251.514347	2907.213987	17.143962	-0.047287	2.972976
251.188995	2899.251346	17.148967	-0.047221	2.969181
251.222940	2891.262498	17.153971	-0.047222	2.965388
251.027549	2883.324890	17.158976	-0.047181	2.961602
250.964382	2875.326971	17.163981	-0.047164	2.957789
251.093614	2867.321926	17.168986	-0.047183	2.953978
251.224319	2859.277983	17.173991	-0.047202	2.950144
251.046174	2851.330702	17.178995	-0.047163	2.946335
250.947603	2843.380607	17.184000	-0.047139	2.942523
251.040804	2835.385548	17.189005	-0.047152	2.938696
250.854670	2827.437743	17.194010	-0.047112	2.934871
250.904955	2819.413618	17.199015	-0.047116	2.931017
250.992034	2811.423881	17.204019	-0.047127	2.927176
250.925019	2803.469852	17.209024	-0.047109	2.923339
250.565258	2795.502767	17.214029	-0.047037	2.919476
250.675323	2787.547164	17.219034	-0.047052	2.915638
250.673693	2779.453045	17.224039	-0.047046	2.911721
250.423425	2771.468037	17.229043	-0.046994	2.907840
250.459716	2763.512376	17.234048	-0.046996	2.903982
250.672116	2755.518261	17.239053	-0.047030	2.900110
250.391380	2747.607904	17.244058	-0.046972	2.896247
250.100143	2739.613974	17.249063	-0.046913	2.892338
250.153074	2731.619640	17.254067	-0.046918	2.888442
250.151055	2723.636432	17.259072	-0.046912	2.884542
249.887352	2715.687450	17.264077	-0.046857	2.880641
250.198714	2707.690258	17.269082	-0.046910	2.876741
250.113986	2699.685066	17.274087	-0.046889	2.872811
250.090670	2691.693524	17.279091	-0.046879	2.868885
250.115656	2683.719566	17.284096	-0.046879	2.864966
250.058055	2675.748053	17.289101	-0.046863	2.861037
249.869726	2667.821226	17.294106	-0.046823	2.857118
249.756059	2659.812917	17.299111	-0.046796	2.853158
249.855496	2651.817574	17.304115	-0.046809	2.849210
249.867974	2643.839324	17.309120	-0.046806	2.845260
249.745352	2635.889353	17.314125	-0.046778	2.841311
249.751862	2627.939602	17.319130	-0.046774	2.837365
249.620762	2619.926840	17.324135	-0.046744	2.833373
249.467507	2611.911676	17.329139	-0.046711	2.829374
249.543495	2603.939317	17.334144	-0.046719	2.825403
249.447566	2595.982791	17.339149	-0.046696	2.821424
249.706829	2587.983121	17.344154	-0.046739	2.817439
249.407811	2580.018820	17.349159	-0.046678	2.813434
249.519993	2572.012535	17.354163	-0.046694	2.809426
249.685562	2564.030105	17.359168	-0.046719	2.805427
249.327470	2556.095167	17.364173	-0.046648	2.801415
249.311523	2548.146511	17.369178	-0.046639	2.797411
249.446501	2540.116930	17.374183	-0.046659	2.793370
249.244368	2532.129322	17.379187	-0.046616	2.789324
249.191449	2524.174949	17.384192	-0.046601	2.785297
249.220102	2516.193673	17.389197	-0.046601	2.781256
249.250528	2508.244684	17.394202	-0.046602	2.777226
249.009779	2500.271920	17.399207	-0.046551	2.773161
249.017868	2492.275150	17.404211	-0.046548	2.769093
249.074480	2484.277097	17.409216	-0.046553	2.765021
248.879949	2476.325745	17.414221	-0.046511	2.760952
248.903599	2468.374026	17.419226	-0.046511	2.756890
248.830414	2460.349091	17.424231	-0.046492	2.752779
248.808897	2452.322791	17.429235	-0.046482	2.748664
248.745178	2444.377926	17.434240	-0.046465	2.744582
248.561235	2436.433034	17.439245	-0.046426	2.740486
248.842351	2428.446866	17.444250	-0.046473	2.736392
248.641149	2420.470407	17.449255	-0.046430	2.732267
248.777324	2412.465420	17.454259	-0.046450	2.728141
248.791194	2404.515971	17.459264	-0.046447	2.724031
248.476712	2396.583919	17.464269	-0.046383	2.719903
248.440193	2388.629698	17.469274	-0.046371	2.715775
248.384474	2380.607024	17.474279	-0.046356	2.711603
248.293675	2372.629706	17.479283	-0.046334	2.707446
248.267121	2364.665361	17.484288	-0.046323	2.703294
248.267292	2356.692722	17.489293	-0.046318	2.699133
248.411701	2348.722776	17.494298	-0.046340	2.694975
248.263701	2340.725810	17.499303	-0.046307	2.690779
248.224566	2332.747890	17.504307	-0.046294	2.686593
248.145938	2324.818681	17.509312	-0.046274	2.682424
247.927464	2316.844056	17.514317	-0.046228	2.678215
247.968144	2308.892100	17.519322	-0.046231	2.674028
247.875258	2300.867118	17.524327	-0.046208	2.669787
247.861582	2292.883664	17.529331	-0.046200	2.665567
247.768433	2284.941403	17.534336	-0.046178	2.661357
247.698367	2276.968346	17.539341	-0.046159	2.657125
247.748420	2268.988055	17.544346	-0.046163	2.652890
247.603274	2261.021507	17.549351	-0.046131	2.648643
247.505355	2253.042409	17.554355	-0.046108	2.644386
247.568816	2245.093510	17.559360	-0.046114	2.640149
247.440929	2237.135936	17.564365	-0.046085	2.635887
247.389228	2229.140542	17.569370	-0.046070	2.631603
247.394747	2221.144440	17.574375	-0.046066	2.627316
247.451772	2213.170698	17.579379	-0.046071	2.623037
247.418737	2205.224270	17.584384	-0.046060	2.618760
247.192591	2197.263554	17.589389	-0.046012	2.614455
247.337186	2189.255585	17.594394	-0.046034	2.610143
247.176442	2181.306821	17.599399	-0.045999	2.605834
247.084847	2173.369591	17.604403	-0.045976	2.601530
247.147668	2165.401553	17.609408	-0.045983	2.597212
247.109478	2157.318402	17.614413	-0.045970	2.592818
247.260634	2149.232438	17.619418	-0.045993	2.588427
247.024669	2141.322489	17.624423	-0.045944	2.584098
247.128248	2133.386442	17.629427	-0.045958	2.579772
247.151860	2125.460583	17.634432	-0.045957	2.575438
246.841703	2117.520342	17.639437	-0.045894	2.571065
246.833955	2109.557067	17.644442	-0.045887	2.566694
246.809021	2101.601304	17.649447	-0.045878	2.562318
246.486777	2093.671268	17.654451	-0.045812	2.557928
246.688433	2085.678196	17.659456	-0.045845	2.553532
246.830694	2077.648445	17.664461	-0.045866	2.549105
246.638506	2069.723514	17.669466	-0.045825	2.544704
246.472700	2061.791329	17.674471	-0.045789	2.540293
246.332974	2053.840495	17.679475	-0.045757	2.535866
246.517150	2045.848822	17.684480	-0.045786	2.531431
246.319217	2037.874011	17.689485	-0.045744	2.526971
246.399248	2029.914105	17.694490	-0.045754	2.522531
246.230822	2021.981901	17.699495	-0.045717	2.518081
246.161848	2013.988990	17.704499	-0.045699	2.513597
246.354440	2005.973124	17.709504	-0.045730	2.509110
246.290984	1997.982828	17.714509	-0.045712	2.504611
246.296225	1990.066148	17.719514	-0.045708	2.500150
246.221123	1982.109869	17.724519	-0.045689	2.495654
246.189273	1974.139209	17.729523	-0.045678	2.491144
246.105077	1966.191431	17.734528	-0.045657	2.486635
245.947543	1958.246199	17.739533	-0.045622	2.482114
246.037342	1950.279823	17.744538	-0.045634	2.477591
245.917371	1942.306231	17.749543	-0.045606	2.473039
245.694236	1934.331048	17.754547	-0.045559	2.468471
245.656161	1926.387242	17.759552	-0.045547	2.463926
245.636395	1918.414605	17.764557	-0.045538	2.459358
245.690024	1910.453156	17.769562	-0.045543	2.454793
245.694051	1902.479075	17.774567	-0.045538	2.450209
245.583864	1894.516767	17.779571	-0.045512	2.445614
245.656342	1886.574378	17.784576	-0.045521	2.441035
245.460002	1878.645828	17.789581	-0.045479	2.436436
245.418136	1870.617502	17.794586	-0.045466	2.431782
245.452493	1862.622976	17.799591	-0.045467	2.427144
245.274347	1854.683610	17.804595	-0.045428	2.422514
245.400201	1846.737994	17.809600	-0.045446	2.417894
245.047255	1838.799937	17.814605	-0.045375	2.413232
245.141958	1830.817159	17.819610	-0.045388	2.408571
245.058596	1822.870798	17.824615	-0.045367	2.403907
245.139210	1814.909023	17.829619	-0.045377	2.399239
245.112051	1806.975210	17.834624	-0.045366	2.394569
244.864407	1798.988989	17.839629	-0.045315	2.389842
245.003534	1791.016337	17.844634	-0.045336	2.385144
245.196697	1783.046781	17.849639	-0.045366	2.380443
244.856199	1775.144995	17.854643	-0.045298	2.375730
244.807994	1767.183595	17.859648	-0.045283	2.370996
244.819176	1759.201313	17.864653	-0.045280	2.366244
244.774221	1751.277120	17.869658	-0.045267	2.361514
244.622001	1743.340517	17.874663	-0.045233	2.356757
244.680993	1735.328733	17.879667	-0.045239	2.351963
244.710683	1727.365521	17.884672	-0.045239	2.347186
244.555197	1719.418959	17.889677	-0.045205	2.342395
244.484263	1711.484259	17.894682	-0.045186	2.337607
244.531056	1703.522476	17.899687	-0.045190	2.332803
244.438131	1695.553551	17.904691	-0.045167	2.327973
244.369541	1687.623100	17.909696	-0.045149	2.323158
244.292690	1679.679970	17.914701	-0.045130	2.318325
244.132821	1671.750452	17.919706	-0.045095	2.313484
244.033925	1663.780984	17.924711	-0.045071	2.308612
244.102803	1655.796721	17.929715	-0.045078	2.303736
244.104443	1647.860675	17.934720	-0.045073	2.298873
244.047632	1639.910847	17.939725	-0.045058	2.293986
243.805382	1631.970321	17.944730	-0.045007	2.289079
244.011584	1623.980600	17.949735	-0.045040	2.284169
243.728349	1616.080520	17.954739	-0.044982	2.279262
243.619212	1608.147634	17.959744	-0.044957	2.274339
243.695914	1600.076137	17.964749	-0.044966	2.269335
243.829102	1592.108538	17.969754	-0.044985	2.264390
243.808748	1584.191560	17.974759	-0.044976	2.259452
243.509783	1576.287447	17.979763	-0.044915	2.254488
243.591063	1568.322359	17.984768	-0.044925	2.249507
243.450107	1560.363835	17.989773	-0.044894	2.244499
243.579520	1552.441933	17.994778	-0.044912	2.239528
243.406917	1544.520373	17.999783	-0.044875	2.234519
243.289072	1536.552998	18.004787	-0.044848	2.229474
243.196761	1528.618365	18.009792	-0.044825	2.224441
243.167545	1520.673477	18.014797	-0.044815	2.219396
243.090112	1512.739713	18.019802	-0.044795	2.214342
243.042960	1504.777045	18.024807	-0.044781	2.209260
242.844134	1496.840184	18.029811	-0.044739	2.204170
243.055518	1488.896752	18.034816	-0.044773	2.199101
242.976221	1480.941395	18.039821	-0.044753	2.193986
243.016317	1472.954301	18.044826	-0.044755	2.188850
242.971242	1465.019491	18.049831	-0.044741	2.183727
243.063305	1457.065048	18.054835	-0.044753	2.178592
242.808133	1449.186070	18.059840	-0.044700	2.173462
242.688196	1441.217820	18.064845	-0.044673	2.168275
242.797566	1433.281291	18.069850	-0.044688	2.163116
242.715353	1425.350801	18.074855	-0.044667	2.157932
242.712366	1417.389493	18.079859	-0.044662	2.152722
242.751586	1409.442831	18.084864	-0.044664	2.147514
242.313598	1401.557672	18.089869	-0.044577	2.142288
242.334978	1393.625934	18.094874	-0.044576	2.137062
242.591455	1385.635912	18.099879	-0.044618	2.131807
242.518431	1377.684760	18.104883	-0.044599	2.126533
242.420344	1369.783742	18.109888	-0.044576	2.121277
242.126830	1361.878779	18.114893	-0.044516	2.115987
242.411510	1353.832742	18.119898	-0.044563	2.110644
242.198188	1345.920553	18.124903	-0.044518	2.105330
242.046998	1337.996709	18.129907	-0.044485	2.100001
242.138229	1330.070450	18.134912	-0.044497	2.094679
241.847078	1322.149216	18.139917	-0.044437	2.089311
241.798236	1314.220243	18.144922	-0.044423	2.083947
241.660645	1306.310813	18.149927	-0.044392	2.078573
241.651821	1298.362999	18.154931	-0.044385	2.073172
241.708061	1290.411510	18.159936	-0.044390	2.067761
241.583054	1282.476893	18.164941	-0.044362	2.062330
241.668576	1274.565007	18.169946	-0.044373	2.056920
241.634138	1266.607636	18.174951	-0.044361	2.051454
241.469273	1258.698311	18.179955	-0.044325	2.045992
241.453534	1250.787854	18.184960	-0.044317	2.040530
241.340214	1242.859987	18.189965	-0.044290	2.035031
241.124323	1234.926038	18.194970	-0.044245	2.029503
241.246064	1226.965635	18.199975	-0.044262	2.023976
240.973216	1219.077073	18.204979	-0.044206	2.018443
241.110009	1211.142418	18.209984	-0.044227	2.012905
240.941316	1203.196485	18.214989	-0.044190	2.007312
241.078031	1195.269411	18.219994	-0.044210	2.001749
241.023327	1187.368567	18.224999	-0.044195	1.996168
240.820287	1179.445564	18.230003	-0.044152	1.990541
240.712796	1171.536597	18.235008	-0.044126	1.984918
240.654593	1163.617349	18.240013	-0.044110	1.979276
240.660536	1155.694746	18.245018	-0.044106	1.973623
240.573011	1147.762380	18.250023	-0.044085	1.967937
240.646858	1139.840359	18.255027	-0.044093	1.962258
240.506283	1131.952285	18.260032	-0.044062	1.956565
240.492997	1123.977273	18.265037	-0.044054	1.950806
240.578110	1116.025011	18.270042	-0.044065	1.945057
240.373023	1108.147725	18.275047	-0.044021	1.939314
240.195659	1100.246727	18.280051	-0.043983	1.933540
240.249582	1092.306003	18.285056	-0.043988	1.927744
240.137780	1084.401114	18.290061	-0.043962	1.921939
240.197413	1076.498296	18.295066	-0.043967	1.916137
240.043554	1068.588415	18.300071	-0.043934	1.910289
240.121509	1060.652566	18.305075	-0.043943	1.904429
240.144184	1052.762455	18.310080	-0.043942	1.898579
239.873925	1044.875320	18.315085	-0.043886	1.892680
239.939341	1036.944394	18.320090	-0.043893	1.886767
239.832655	1029.059648	18.325095	-0.043868	1.880852
239.706459	1021.165391	18.330099	-0.043839	1.874908
239.789980	1013.226383	18.335104	-0.043850	1.868935
239.778584	1005.302613	18.340109	-0.043842	1.862944
239.714724	997.412950	18.345114	-0.043825	1.856953
239.457800	989.533070	18.350119	-0.043772	1.850928
239.669580	981.581419	18.355123	-0.043806	1.844883
239.416577	973.734105	18.360128	-0.043754	1.838844
239.277224	965.841327	18.365133	-0.043723	1.832763
239.339520	957.918515	18.370138	-0.043729	1.826663
239.321918	950.023711	18.375143	-0.043721	1.820554
239.260679	942.133802	18.380147	-0.043704	1.814423
239.310466	934.221997	18.385152	-0.043708	1.808268
239.035537	926.366542	18.390157	-0.043652	1.802097
239.048040	918.478375	18.395162	-0.043649	1.795913
238.837430	910.547548	18.400167	-0.043604	1.789648
238.749721	902.641546	18.405171	-0.043583	1.783394
238.810026	894.759961	18.410176	-0.043589	1.777157
238.705319	886.863826	18.415181	-0.043564	1.770866
238.609952	878.978725	18.420186	-0.043541	1.764562
238.694895	871.097597	18.425191	-0.043552	1.758261
238.429224	863.228221	18.430195	-0.043497	1.751903
238.459904	855.330053	18.435200	-0.043497	1.745535
238.628277	847.425972	18.440205	-0.043524	1.739158
238.609639	839.553920	18.445210	-0.043515	1.732759
238.399388	831.700307	18.450215	-0.043471	1.726326
238.225773	823.839523	18.455219	-0.043433	1.719869
238.416619	815.948363	18.460224	-0.043463	1.713409
238.166840	808.066809	18.465229	-0.043412	1.706876
238.145622	800.187090	18.470234	-0.043402	1.700348
238.177982	792.314136	18.475239	-0.043403	1.693808
237.976690	784.445715	18.480243	-0.043361	1.687216
238.018522	776.576203	18.485248	-0.043363	1.680629
237.962389	768.716850	18.490253	-0.043347	1.674012
237.838172	760.848450	18.495258	-0.043319	1.667352
237.824773	752.984206	18.500263	-0.043311	1.660683
237.796125	745.120434	18.505267	-0.043301	1.653986
237.892285	737.234329	18.510272	-0.043314	1.647260
237.610323	729.412253	18.515277	-0.043256	1.640509
237.767652	721.527154	18.520282	-0.043280	1.633736
237.567348	713.642214	18.525287	-0.043237	1.626886
237.278727	705.817670	18.530291	-0.043178	1.620047
237.331599	697.963829	18.535296	-0.043183	1.613201
237.256754	690.087613	18.540301	-0.043164	1.606288
237.143090	682.265705	18.545306	-0.043138	1.599388
237.049272	674.432119	18.550311	-0.043115	1.592450
236.929283	666.568314	18.555315	-0.043087	1.585451
237.037534	658.727127	18.560320	-0.043102	1.578474
236.858278	650.887515	18.565325	-0.043064	1.571427
236.834680	643.044197	18.570330	-0.043054	1.564366
236.918818	635.209676	18.575335	-0.043065	1.557297
236.807493	627.355409	18.580339	-0.043039	1.550150
236.705311	619.535075	18.585344	-0.043015	1.543001
236.708877	611.692721	18.590349	-0.043010	1.535815
236.624883	603.866876	18.595354	-0.042989	1.528597
236.483174	596.063321	18.600359	-0.042958	1.521357
236.351407	588.256332	18.605363	-0.042928	1.514080
236.445768	580.405211	18.610368	-0.042940	1.506762
236.236088	572.612802	18.615373	-0.042896	1.499416
236.331906	564.772147	18.620378	-0.042909	1.492036
236.293976	556.955165	18.625383	-0.042896	1.484620
236.247080	549.155119	18.630387	-0.042883	1.477182
235.971336	541.353140	18.635392	-0.042826	1.469669
236.069904	533.501189	18.640397	-0.042839	1.462128
235.831974	525.741140	18.645402	-0.042790	1.454583
235.652791	517.948145	18.650407	-0.042751	1.446976
235.510003	510.161261	18.655411	-0.042719	1.439341
235.666539	502.345476	18.660416	-0.042743	1.431686
235.655419	494.541207	18.665421	-0.042736	1.423973
235.562336	486.767285	18.670426	-0.042714	1.416234
235.444968	478.992964	18.675431	-0.042687	1.408449
235.429179	471.197712	18.680435	-0.042679	1.400617
235.196594	463.470989	18.685440	-0.042630	1.392773
235.183656	455.654801	18.690445	-0.042623	1.384831
235.318095	447.861120	18.695450	-0.042642	1.376891
235.157864	440.106458	18.700455	-0.042607	1.368895
235.039527	432.354518	18.705459	-0.042580	1.360861
234.822680	424.641161	18.710464	-0.042535	1.352803
234.818562	416.853578	18.715469	-0.042529	1.344657
234.714591	409.121247	18.720474	-0.042504	1.336501
234.694148	401.360769	18.725479	-0.042495	1.328280
234.620330	393.621668	18.730483	-0.042477	1.320021
234.553934	385.835299	18.735488	-0.042459	1.311660
234.467355	378.032971	18.740493	-0.042438	1.303225
234.422277	370.316116	18.745498	-0.042424	1.294836
234.318705	362.604934	18.750503	-0.042400	1.286387
234.150094	354.916473	18.755507	-0.042363	1.277896
234.227405	347.187143	18.760512	-0.042373	1.269348
234.001421	339.502220	18.765517	-0.042325	1.260734
233.835847	331.821804	18.770522	-0.042290	1.252078
233.805902	324.114932	18.775527	-0.042279	1.243358
233.910320	316.403150	18.780531	-0.042293	1.234596
233.699742	308.732664	18.785536	-0.042249	1.225758
233.471775	301.075415	18.790541	-0.042201	1.216867
233.712073	293.344087	18.795546	-0.042241	1.207918
233.663105	285.687046	18.800551	-0.042227	1.198931
233.284175	278.080502	18.805555	-0.042151	1.189869
233.367355	270.399989	18.810560	-0.042162	1.180743
233.308040	262.753683	18.815565	-0.042146	1.171559
233.188673	255.123710	18.820570	-0.042118	1.162309
233.086875	247.496892	18.825575	-0.042094	1.152992
232.869334	239.850944	18.830579	-0.042049	1.143551
232.897822	232.231021	18.835584	-0.042049	1.134117
232.695701	224.629164	18.840589	-0.042006	1.124576
232.696371	217.023006	18.845594	-0.042001	1.114992
232.602524	209.429916	18.850599	-0.041979	1.105321
232.435339	201.865363	18.855603	-0.041943	1.095586
232.560774	194.253163	18.860608	-0.041961	1.085766
232.523112	186.692897	18.865613	-0.041949	1.075888
232.105379	179.180915	18.870618	-0.041866	1.065895
232.107811	171.625082	18.875623	-0.041862	1.055846
232.085318	164.068610	18.880627	-0.041852	1.045694
232.064243	156.552305	18.885632	-0.041844	1.035498
231.488008	149.112053	18.890637	-0.041731	1.025172
231.431697	141.606653	18.895642	-0.041716	1.014775
231.488395	134.089291	18.900647	-0.041721	1.004282
231.286320	126.627875	18.905651	-0.041679	0.993694
231.445748	119.094001	18.910656	-0.041704	0.982977
231.240698	111.662872	18.915661	-0.041660	0.972200
231.075310	104.240109	18.920666	-0.041625	0.961324
231.005127	96.824572	18.925671	-0.041607	0.950359
230.735207	89.442867	18.930675	-0.041552	0.939264
230.717065	82.042910	18.935680	-0.041543	0.928076
230.558311	74.685738	18.940685	-0.041509	0.916779
230.483255	67.315345	18.945690	-0.041490	0.905343
230.373862	60.215250	18.950695	-0.041465	0.894178