Fri Mar 12 11:10:59 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.439674	0.012928	0.000000	0.000057	0.717378
0.620276	-0.023212	0.005005	0.000024	0.717370
0.552319	-0.010107	0.010010	0.000037	0.717371
0.727604	-0.037368	0.015014	0.000004	0.717379
0.710760	-0.039325	0.020019	0.000008	0.717368
0.604066	-0.016241	0.025024	0.000028	0.717376
0.542806	-0.005039	0.030029	0.000039	0.717376
0.460192	0.007639	0.035034	0.000055	0.717372
0.522820	0.001313	0.040038	0.000043	0.717381
0.524772	-0.002966	0.045043	0.000043	0.717373
0.518242	0.002039	0.050048	0.000045	0.717380
0.714673	-0.034789	0.055053	0.000008	0.717376
0.683679	-0.030201	0.060058	0.000014	0.717374
0.808088	-0.048440	0.065062	-0.000009	0.717381
0.611720	-0.017591	0.070067	0.000028	0.717372
0.810761	-0.048965	0.075072	-0.000009	0.717380
0.842019	-0.129765	0.080077	-0.000014	0.717231
0.703650	-0.185028	0.085082	0.000012	0.717072
0.704169	-0.181122	0.090086	0.000012	0.717080
0.696539	-0.183771	0.095091	0.000014	0.717071
0.708573	-0.182271	0.100096	0.000012	0.717078
0.425653	-0.131822	0.105101	0.000064	0.717078
0.503572	-0.148842	0.110106	0.000050	0.717071
0.451990	-0.295295	0.115110	0.000060	0.716763
0.343487	-0.285730	0.120115	0.000081	0.716743
0.537761	-0.316221	0.125120	0.000045	0.716751
0.489328	-0.308643	0.130125	0.000054	0.716748
0.518835	-0.312544	0.135130	0.000049	0.716750
0.514456	-0.420276	0.140134	0.000050	0.716535
0.343653	-0.439850	0.145139	0.000082	0.716436
0.268292	-0.423061	0.150144	0.000096	0.716442
0.280991	-0.427003	0.155149	0.000094	0.716438
0.492231	-0.502409	0.160154	0.000055	0.716363
0.543555	-0.630641	0.165158	0.000045	0.716127
0.382828	-0.604910	0.170163	0.000076	0.716121
0.424635	-0.610570	0.175168	0.000068	0.716124
0.554450	-0.687565	0.180173	0.000044	0.716016
0.541479	-0.755577	0.185178	0.000047	0.715877
0.377006	-0.722522	0.190182	0.000078	0.715884
0.301954	-0.715241	0.195187	0.000092	0.715871
0.234689	-0.868320	0.200192	0.000105	0.715544
0.367970	-0.892245	0.205197	0.000080	0.715543
0.297495	-0.883099	0.210202	0.000093	0.715536
0.356135	-1.015802	0.215206	0.000083	0.715293
0.266439	-1.036162	0.220211	0.000100	0.715220
0.472079	-1.070342	0.225216	0.000062	0.715225
0.326720	-1.181870	0.230221	0.000089	0.714952
0.329244	-1.210423	0.235226	0.000089	0.714895
0.489971	-1.248479	0.240230	0.000059	0.714876
0.317732	-1.358138	0.245235	0.000092	0.714597
0.356081	-1.361810	0.250240	0.000085	0.714603
0.298147	-1.430633	0.255245	0.000096	0.714445
0.244475	-1.511238	0.260250	0.000106	0.714266
0.300577	-1.516031	0.265254	0.000096	0.714276
-0.090198	-1.603366	0.270259	0.000169	0.713964
-0.079841	-1.606413	0.275264	0.000167	0.713961
0.039724	-1.699327	0.280269	0.000145	0.713818
0.070272	-1.793836	0.285274	0.000140	0.713641
0.031011	-1.800015	0.290278	0.000147	0.713614
-0.238441	-1.885038	0.295283	0.000198	0.713349
-0.214211	-1.886396	0.300288	0.000193	0.713354
-0.033547	-2.049136	0.305293	0.000160	0.713094
-0.007219	-2.092367	0.310298	0.000155	0.713017
-0.079554	-2.170053	0.315302	0.000169	0.712836
-0.294254	-2.200983	0.320307	0.000209	0.712698
-0.159973	-2.293650	0.325312	0.000185	0.712561
-1.781827	-2.094749	0.330317	0.000487	0.712381
-1.889152	-2.077607	0.335322	0.000507	0.712377
-2.298439	-2.138961	0.340326	0.000583	0.712109
-3.083302	-2.014094	0.345331	0.000730	0.712079
-2.565557	-2.110955	0.350336	0.000634	0.712069
-2.889782	-2.211481	0.355341	0.000694	0.711753
-3.880110	-2.036486	0.360346	0.000879	0.711750
-3.680372	-2.066776	0.365350	0.000842	0.711760
-3.770439	-2.192518	0.370355	0.000859	0.711477
-4.503582	-2.074499	0.375360	0.000995	0.711451
-4.709278	-2.039512	0.380365	0.001034	0.711447
-4.329018	-2.177840	0.385370	0.000964	0.711306
-5.354379	-2.079955	0.390374	0.001155	0.711136
-5.462401	-2.065656	0.395379	0.001175	0.711126
-5.385622	-2.076897	0.400384	0.001161	0.711131
-5.551445	-2.114754	0.405389	0.001192	0.710996
-6.668130	-1.984912	0.410394	0.001400	0.710857
-5.927217	-2.110438	0.415398	0.001262	0.710870
-6.161817	-2.074167	0.420403	0.001306	0.710858
-6.236092	-2.095513	0.425408	0.001320	0.710789
-7.265182	-2.042809	0.430413	0.001512	0.710527
-6.982208	-2.095448	0.435418	0.001460	0.710523
-6.950906	-2.098547	0.440422	0.001454	0.710527
-7.397859	-2.022242	0.445427	0.001537	0.710520
-7.260647	-2.103686	0.450432	0.001512	0.710406
-7.944295	-2.081063	0.455437	0.001640	0.710207
-7.825148	-2.104310	0.460442	0.001618	0.710203
-8.115793	-2.046482	0.465446	0.001672	0.710214
-8.313602	-2.015667	0.470451	0.001709	0.710205
-7.965221	-2.114214	0.475456	0.001645	0.710132
-8.960645	-2.060973	0.480461	0.001830	0.709883
-8.932353	-2.067247	0.485466	0.001825	0.709880
-8.692450	-2.106861	0.490470	0.001781	0.709886
-8.929566	-2.066656	0.495475	0.001825	0.709882
-8.969767	-2.057796	0.500480	0.001833	0.709885
-8.893244	-2.156203	0.505485	0.001819	0.709715
-10.226985	-1.984291	0.510490	0.002067	0.709583
-9.755654	-2.064566	0.515494	0.001980	0.709590
-9.655983	-2.086527	0.520499	0.001961	0.709581
-9.961699	-2.029528	0.525504	0.002018	0.709585
-10.000552	-2.020480	0.530509	0.002026	0.709589
-10.004562	-2.102000	0.535514	0.002027	0.709424
-10.527337	-2.090227	0.540518	0.002124	0.709261
-10.398740	-2.116873	0.545523	0.002101	0.709253
-10.833885	-2.036651	0.550528	0.002182	0.709258
-10.432941	-2.108676	0.555533	0.002108	0.709257
-10.508540	-2.096941	0.560538	0.002122	0.709253
-10.749965	-2.137707	0.565542	0.002167	0.709085
-11.738405	-2.029642	0.570547	0.002351	0.708948
-11.190124	-2.126173	0.575552	0.002249	0.708950
-11.445017	-2.080181	0.580557	0.002297	0.708950
-11.801702	-2.018699	0.585562	0.002364	0.708946
-11.131159	-2.135149	0.590566	0.002239	0.708952
-11.620545	-2.085726	0.595571	0.002330	0.708875
-12.660910	-2.021773	0.600576	0.002524	0.708632
-12.254567	-2.092580	0.605581	0.002449	0.708635
-12.518033	-2.048567	0.610586	0.002498	0.708628
-12.309917	-2.082837	0.615590	0.002460	0.708633
-12.124656	-2.118683	0.620595	0.002425	0.708627
-12.477601	-2.054514	0.625600	0.002491	0.708629
-12.720108	-2.101240	0.630605	0.002537	0.708449
-13.615531	-1.997919	0.635610	0.002704	0.708336
-12.967334	-2.107238	0.640614	0.002583	0.708348
-13.297916	-2.053909	0.645619	0.002645	0.708336
-13.732749	-1.973313	0.650624	0.002726	0.708342
-13.119521	-2.080490	0.655629	0.002612	0.708346
-13.005805	-2.104168	0.660634	0.002591	0.708338
-13.815610	-2.093004	0.665638	0.002742	0.708071
-14.647187	-1.978719	0.670643	0.002897	0.708003
-14.235629	-2.049994	0.675648	0.002821	0.708006
-14.076475	-2.076358	0.680653	0.002791	0.708010
-14.674104	-1.974259	0.685658	0.002903	0.708001
-13.983035	-2.092744	0.690662	0.002775	0.708010
-13.977966	-2.098613	0.695667	0.002774	0.707999
-14.608760	-2.094533	0.700672	0.002891	0.707782
-15.225629	-2.027646	0.705677	0.003007	0.707695
-15.213570	-2.034175	0.710682	0.003005	0.707686
-15.023479	-2.060763	0.715686	0.002969	0.707700
-15.517623	-1.977688	0.720691	0.003062	0.707689
-14.936088	-2.078795	0.725696	0.002954	0.707694
-15.026337	-2.062535	0.730701	0.002971	0.707694
-15.737939	-2.026727	0.735706	0.003103	0.707511
-15.990761	-2.048554	0.740710	0.003151	0.707376
-15.867342	-2.075708	0.745715	0.003128	0.707366
-16.163640	-2.021749	0.750720	0.003183	0.707367
-15.964468	-2.054665	0.755725	0.003146	0.707372
-15.925223	-2.064560	0.760730	0.003139	0.707366
-16.318792	-1.990968	0.765734	0.003213	0.707372
-16.552666	-1.975206	0.770739	0.003256	0.707320
-16.463424	-2.113274	0.775744	0.003240	0.707074
-16.358276	-2.131143	0.780749	0.003221	0.707076
-17.558844	-1.920042	0.785754	0.003444	0.707069
-16.929248	-2.028633	0.790758	0.003328	0.707076
-16.770668	-2.057737	0.795763	0.003298	0.707074
-17.129203	-1.992295	0.800768	0.003365	0.707077
-17.017144	-2.058164	0.805773	0.003345	0.706984
-17.843640	-2.031347	0.810778	0.003499	0.706742
-17.555872	-2.078272	0.815782	0.003445	0.706750
-17.992415	-2.005802	0.820787	0.003527	0.706739
-17.821458	-2.035247	0.825792	0.003495	0.706741
-17.507907	-2.086302	0.830797	0.003437	0.706750
-17.879195	-2.023560	0.835802	0.003506	0.706743
-17.584329	-2.135514	0.840806	0.003452	0.706623
-18.627566	-2.044632	0.845811	0.003646	0.706431
-18.771826	-2.018238	0.850816	0.003673	0.706432
-18.846633	-2.001662	0.855821	0.003687	0.706438
-18.694540	-2.031707	0.860826	0.003659	0.706432
-18.365248	-2.085416	0.865830	0.003598	0.706442
-18.881188	-1.997041	0.870835	0.003694	0.706434
-18.859976	-2.056770	0.875840	0.003691	0.706321
-19.328407	-2.072071	0.880845	0.003778	0.706122
-19.672059	-2.014754	0.885850	0.003842	0.706114
-19.766010	-1.991893	0.890854	0.003860	0.706126
-19.380500	-2.064012	0.895859	0.003789	0.706118
-19.608878	-2.022352	0.900864	0.003831	0.706120
-19.670732	-2.009755	0.905869	0.003843	0.706123
-19.707437	-2.028583	0.910874	0.003850	0.706071
-20.025149	-2.076535	0.915878	0.003910	0.705861
-20.232226	-2.042940	0.920883	0.003948	0.705853
-20.480412	-1.998602	0.925888	0.003995	0.705853
-19.902796	-2.098020	0.930893	0.003887	0.705860
-20.416192	-2.009432	0.935898	0.003983	0.705854
-20.073705	-2.065072	0.940902	0.003920	0.705864
-20.131720	-2.182952	0.945907	0.003931	0.705606
-21.516438	-1.978095	0.950912	0.004189	0.705521
-21.548304	-1.970379	0.955917	0.004195	0.705524
-21.232775	-2.031614	0.960922	0.004136	0.705514
-21.083466	-2.053170	0.965926	0.004109	0.705524
-21.390847	-2.003631	0.970931	0.004166	0.705513
-21.137873	-2.047818	0.975936	0.004119	0.705514
-21.080640	-2.183888	0.980941	0.004109	0.705260
-22.256211	-2.005007	0.985946	0.004328	0.705198
-22.219573	-2.005472	0.990950	0.004321	0.705210
-22.098879	-2.030847	0.995955	0.004299	0.705202
-22.046816	-2.039025	1.000960	0.004290	0.705204
-22.097783	-2.027865	1.005965	0.004299	0.705207
-22.107452	-2.028760	1.010970	0.004301	0.705202
-22.241936	-2.161752	1.015974	0.004327	0.704885
-23.157420	-2.002594	1.020979	0.004497	0.704877
-23.326900	-1.971432	1.025984	0.004529	0.704878
-22.642693	-2.092034	1.030989	0.004402	0.704880
-23.019430	-2.027527	1.035994	0.004472	0.704875
-23.016059	-2.022955	1.040998	0.004472	0.704885
-22.740058	-2.093183	1.046003	0.004421	0.704842
-23.710060	-2.050023	1.051008	0.004602	0.704580
-23.991269	-1.996578	1.056013	0.004654	0.704586
-24.357345	-1.934201	1.061018	0.004723	0.704580
-23.508370	-2.082167	1.066022	0.004565	0.704586
-23.859446	-2.022348	1.071027	0.004630	0.704580
-24.017311	-1.992946	1.076032	0.004660	0.704582
-23.438810	-2.106327	1.081037	0.004553	0.704561
-24.522149	-2.068805	1.086042	0.004754	0.704247
-24.849075	-2.006862	1.091046	0.004815	0.704254
-25.033362	-1.976814	1.096051	0.004850	0.704248
-24.529368	-2.066339	1.101056	0.004756	0.704248
-24.752231	-2.024807	1.106061	0.004798	0.704252
-25.141784	-1.957080	1.111066	0.004871	0.704248
-24.360307	-2.093327	1.116070	0.004726	0.704253
-25.201135	-2.090414	1.121075	0.004882	0.703957
-25.948222	-1.965751	1.126080	0.005022	0.703939
-25.418754	-2.054209	1.131085	0.004923	0.703951
-25.386727	-2.064119	1.136090	0.004918	0.703942
-25.861095	-1.976198	1.141094	0.005006	0.703948
-25.598541	-2.025737	1.146099	0.004957	0.703942
-25.248386	-2.093990	1.151104	0.004893	0.703930
-26.154502	-2.080252	1.156109	0.005061	0.703631
-26.654940	-1.994606	1.161114	0.005155	0.703624
-26.261935	-2.060712	1.166118	0.005082	0.703631
-26.233187	-2.070344	1.171123	0.005077	0.703622
-26.662998	-1.990947	1.176128	0.005157	0.703627
-26.312214	-2.052735	1.181133	0.005092	0.703628
-26.320425	-2.092329	1.186138	0.005094	0.703545
-27.353739	-2.011517	1.191142	0.005286	0.703335
-27.074572	-2.062780	1.196147	0.005235	0.703332
-27.208358	-2.038057	1.201152	0.005260	0.703333
-27.158398	-2.043002	1.206157	0.005251	0.703341
-27.417637	-2.002369	1.211162	0.005299	0.703329
-27.096883	-2.053932	1.216166	0.005240	0.703340
-27.384139	-2.086819	1.221171	0.005293	0.703170
-28.502621	-1.972442	1.226176	0.005502	0.702998
-28.025197	-2.055809	1.231181	0.005413	0.703001
-28.219244	-2.023974	1.236186	0.005449	0.702995
-28.542830	-1.962473	1.241190	0.005510	0.703002
-28.319931	-2.003510	1.246195	0.005469	0.702999
-28.221016	-2.021785	1.251200	0.005450	0.702997
-27.859020	-2.131984	1.256205	0.005383	0.702905
-29.240257	-1.996330	1.261210	0.005641	0.702681
-28.942166	-2.045406	1.266214	0.005585	0.702689
-29.304721	-1.982481	1.271219	0.005653	0.702685
-29.489724	-1.948432	1.276224	0.005688	0.702686
-29.061227	-2.023000	1.281229	0.005608	0.702690
-29.087811	-2.021756	1.286234	0.005613	0.702682
-29.033893	-2.045371	1.291238	0.005604	0.702653
-29.975593	-2.021169	1.296243	0.005779	0.702363
-29.850169	-2.042202	1.301248	0.005756	0.702365
-29.754317	-2.058347	1.306253	0.005738	0.702366
-30.091394	-2.001892	1.311258	0.005801	0.702358
-29.670716	-2.072096	1.316262	0.005723	0.702368
-29.590369	-2.087754	1.321267	0.005709	0.702365
-29.979984	-2.081883	1.326272	0.005781	0.702236
-30.745222	-2.026812	1.331277	0.005924	0.702071
-30.463810	-2.081371	1.336282	0.005872	0.702061
-30.598646	-2.053180	1.341286	0.005897	0.702069
-30.816546	-2.016468	1.346291	0.005938	0.702065
-30.830224	-2.013701	1.351296	0.005941	0.702065
-30.479017	-2.073720	1.356301	0.005876	0.702070
-31.341613	-2.047291	1.361306	0.006036	0.701812
-31.742861	-2.010054	1.366310	0.006111	0.701742
-31.666680	-2.026396	1.371315	0.006097	0.701736
-31.897587	-1.985511	1.376320	0.006141	0.701735
-31.948709	-1.973946	1.381325	0.006150	0.701739
-31.492393	-2.056798	1.386330	0.006066	0.701736
-31.428519	-2.064813	1.391334	0.006054	0.701742
-31.878053	-2.067091	1.396339	0.006138	0.701575
-32.897270	-1.957083	1.401344	0.006328	0.701429
-32.175276	-2.082300	1.406349	0.006194	0.701436
-32.763597	-1.982268	1.411354	0.006303	0.701426
-32.832181	-1.967089	1.416358	0.006316	0.701431
-32.321803	-2.059622	1.421363	0.006222	0.701428
-32.468360	-2.033006	1.426368	0.006249	0.701428
-32.677792	-2.079677	1.431373	0.006288	0.701258
-33.710077	-1.969227	1.436378	0.006481	0.701108
-33.468555	-2.009155	1.441382	0.006436	0.701114
-33.529346	-1.999105	1.446387	0.006447	0.701112
-33.385381	-2.023408	1.451392	0.006421	0.701114
-33.182425	-2.057114	1.456397	0.006383	0.701119
-33.673227	-1.974429	1.461402	0.006475	0.701109
-33.379698	-2.080620	1.466406	0.006421	0.700999
-33.888035	-2.055753	1.471411	0.006515	0.700866
-34.149632	-2.009392	1.476416	0.006564	0.700865
-34.161930	-2.003019	1.481421	0.006567	0.700873
-34.178671	-2.005330	1.486426	0.006570	0.700861
-33.924919	-2.047479	1.491430	0.006523	0.700867
-34.283592	-1.990548	1.496435	0.006590	0.700853
-34.847284	-2.052368	1.501440	0.006695	0.700523
-34.730016	-2.069218	1.506445	0.006674	0.700531
-35.182542	-1.994237	1.511450	0.006758	0.700519
-34.929091	-2.034641	1.516454	0.006711	0.700528
-34.839256	-2.053914	1.521459	0.006695	0.700521
-34.988267	-2.026012	1.526464	0.006723	0.700523
-34.874437	-2.115934	1.531469	0.006702	0.700382
-36.292177	-1.950723	1.536474	0.006966	0.700204
-35.835473	-2.026568	1.541478	0.006881	0.700215
-35.865833	-2.022558	1.546483	0.006887	0.700211
-35.993155	-2.003219	1.551488	0.006911	0.700204
-35.546686	-2.077663	1.556493	0.006828	0.700214
-36.152867	-1.974005	1.561498	0.006941	0.700205
-36.223895	-2.046393	1.566502	0.006955	0.700032
-36.736087	-2.026045	1.571507	0.007050	0.699887
-36.613878	-2.049050	1.576512	0.007028	0.699884
-36.701292	-2.029979	1.581517	0.007044	0.699891
-36.845301	-2.007123	1.586522	0.007071	0.699885
-36.606272	-2.047539	1.591526	0.007027	0.699889
-36.814010	-2.012895	1.596531	0.007066	0.699884
-37.111153	-2.069373	1.601536	0.007121	0.699661
-37.313802	-2.064704	1.606541	0.007159	0.699597
-37.505362	-2.036057	1.611546	0.007195	0.699585
-37.508461	-2.030602	1.616550	0.007196	0.699595
-37.621581	-2.009831	1.621555	0.007217	0.699595
-37.545576	-2.026403	1.626560	0.007203	0.699589
-37.444200	-2.064801	1.631565	0.007185	0.699547
-38.524675	-2.015801	1.636570	0.007386	0.699255
-38.309400	-2.050985	1.641574	0.007346	0.699261
-38.650128	-1.990082	1.646579	0.007410	0.699261
-38.523510	-2.013566	1.651584	0.007386	0.699259
-37.815456	-2.135058	1.656589	0.007255	0.699268
-38.785028	-1.967961	1.661594	0.007436	0.699256
-38.631156	-2.030966	1.666598	0.007407	0.699183
-39.090027	-2.063209	1.671603	0.007493	0.698951
-39.217949	-2.042601	1.676608	0.007517	0.698946
-39.415343	-2.001077	1.681613	0.007554	0.698958
-39.393526	-2.011170	1.686618	0.007550	0.698945
-39.039596	-2.068934	1.691622	0.007484	0.698956
-39.348038	-2.018321	1.696627	0.007542	0.698946
-39.488594	-2.057410	1.701632	0.007568	0.698816
-40.056403	-2.045012	1.706637	0.007674	0.698634
-39.764960	-2.101771	1.711642	0.007620	0.698624
-40.273856	-2.006726	1.716646	0.007715	0.698633
-40.312089	-2.001000	1.721651	0.007723	0.698630
-40.055639	-2.048484	1.726656	0.007675	0.698626
-40.039182	-2.046677	1.731661	0.007672	0.698635
-40.381024	-2.090292	1.736666	0.007736	0.698422
-41.050047	-2.009556	1.741670	0.007861	0.698343
-40.959709	-2.024957	1.746675	0.007844	0.698344
-41.219432	-1.980801	1.751680	0.007893	0.698339
-40.943877	-2.026474	1.756685	0.007842	0.698346
-41.124699	-1.996928	1.761690	0.007876	0.698340
-41.099568	-1.997514	1.766694	0.007871	0.698348
-41.175570	-2.104571	1.771699	0.007886	0.698102
-42.083032	-1.991489	1.776704	0.008055	0.698002
-41.862086	-2.026427	1.781709	0.008014	0.698011
-42.223166	-1.966722	1.786714	0.008081	0.698001
-41.930306	-2.016520	1.791718	0.008027	0.698005
-41.932679	-2.014542	1.796723	0.008028	0.698008
-42.088867	-1.988965	1.801728	0.008057	0.698003
-41.938533	-2.107724	1.806733	0.008029	0.697815
-42.545582	-2.061390	1.811738	0.008143	0.697689
-42.623312	-2.043172	1.816742	0.008157	0.697697
-42.843483	-2.004456	1.821747	0.008198	0.697696
-42.981261	-1.982238	1.826752	0.008224	0.697691
-42.780707	-2.012468	1.831757	0.008187	0.697701
-43.018117	-1.975547	1.836762	0.008232	0.697690
-43.082575	-2.085539	1.841766	0.008244	0.697442
-43.779996	-1.997527	1.846771	0.008374	0.697368
-44.087176	-1.944517	1.851776	0.008431	0.697364
-43.646454	-2.018125	1.856781	0.008349	0.697373
-43.798161	-1.996371	1.861786	0.008378	0.697362
-43.930874	-1.969192	1.866790	0.008403	0.697369
-43.711951	-2.008066	1.871795	0.008362	0.697369
-43.654406	-2.093102	1.876800	0.008352	0.697216
-44.644606	-1.982846	1.881805	0.008536	0.697080
-44.724407	-1.973876	1.886810	0.008551	0.697069
-44.609724	-1.991133	1.891814	0.008530	0.697075
-44.360554	-2.035940	1.896819	0.008484	0.697074
-44.513850	-2.011295	1.901824	0.008513	0.697068
-44.457705	-2.016233	1.906829	0.008503	0.697078
-44.686714	-2.088913	1.911834	0.008546	0.696846
-45.586292	-1.977322	1.916838	0.008713	0.696746
-45.516045	-1.989794	1.921843	0.008700	0.696746
-45.288917	-2.034001	1.926848	0.008658	0.696738
-45.292039	-2.027489	1.931853	0.008659	0.696750
-45.699941	-1.958728	1.936858	0.008735	0.696741
-45.298564	-2.026321	1.941862	0.008661	0.696749
-45.638237	-2.072162	1.946867	0.008724	0.696531
-46.785667	-1.915147	1.951872	0.008938	0.696434
-46.310209	-1.995346	1.956877	0.008850	0.696443
-46.246737	-2.010818	1.961882	0.008838	0.696434
-46.420634	-1.976257	1.966886	0.008871	0.696440
-46.430270	-1.974517	1.971891	0.008873	0.696440
-46.173530	-2.022475	1.976896	0.008825	0.696435
-46.148423	-2.122891	1.981901	0.008821	0.696239
-47.669359	-1.910545	1.986906	0.009104	0.696118
-47.154481	-1.999769	1.991910	0.009009	0.696123
-46.813470	-2.060311	1.996915	0.008945	0.696123
-47.369571	-1.960593	2.001920	0.009049	0.696124
-47.188089	-1.992504	2.011917	0.009016	0.696124
-47.709401	-1.987962	2.021914	0.009113	0.695943
-47.620713	-2.039040	2.031910	0.009097	0.695870
-47.570986	-2.046836	2.041907	0.009088	0.695871
-47.788149	-2.007826	2.051904	0.009129	0.695871
-47.488541	-2.061384	2.061901	0.009074	0.695870
-47.891001	-1.990047	2.071898	0.009149	0.695868
-47.753437	-2.012784	2.081894	0.009124	0.695871
-47.636959	-2.033138	2.091891	0.009103	0.695871
-47.302546	-2.000898	2.101888	0.009041	0.696058
-47.151831	-1.998217	2.111885	0.009013	0.696117
-47.178614	-1.991636	2.121882	0.009019	0.696120
-47.052064	-2.013518	2.131878	0.008996	0.696120
-47.017856	-2.018507	2.141875	0.008990	0.696122
-47.066899	-2.009603	2.151872	0.008999	0.696121
-46.864921	-1.978258	2.161869	0.008962	0.696258
-46.408550	-1.972239	2.171866	0.008878	0.696435
-46.227781	-2.003027	2.181862	0.008844	0.696437
-46.238377	-2.000712	2.191859	0.008847	0.696437
-46.255468	-1.988274	2.201856	0.008851	0.696456
-45.362217	-2.005154	2.211853	0.008685	0.696745
-45.321147	-2.012784	2.221850	0.008677	0.696744
-44.996701	-2.067282	2.231846	0.008618	0.696750
-45.261115	-2.020421	2.241843	0.008667	0.696748
-44.745047	-1.990013	2.251840	0.008571	0.696997
-44.529049	-1.990649	2.261837	0.008532	0.697074
-44.501775	-1.995052	2.271834	0.008527	0.697074
-44.025712	-2.078547	2.281830	0.008439	0.697076
-43.744653	-2.003778	2.291827	0.008387	0.697329
-43.541582	-2.018857	2.301824	0.008350	0.697371
-43.565922	-2.015281	2.311821	0.008355	0.697369
-43.614095	-1.977256	2.321818	0.008364	0.697428
-42.627078	-2.022314	2.331814	0.008181	0.697694
-42.825481	-1.986464	2.341811	0.008218	0.697694
-42.551066	-2.035216	2.351808	0.008167	0.697694
-42.196303	-1.993944	2.361805	0.008102	0.697906
-41.946430	-1.987665	2.371802	0.008056	0.698008
-41.494465	-2.066394	2.381798	0.007972	0.698011
-41.636796	-2.040161	2.391795	0.007999	0.698012
-40.960443	-2.014088	2.401792	0.007873	0.698310
-41.114984	-1.969386	2.411789	0.007903	0.698344
-40.822236	-2.021022	2.421786	0.007849	0.698344
-40.716660	-1.987896	2.431782	0.007829	0.698449
-39.890371	-2.042788	2.441779	0.007676	0.698636
-39.838420	-2.052552	2.451776	0.007667	0.698634
-40.210051	-1.985116	2.461773	0.007736	0.698635
-39.431197	-1.998181	2.471770	0.007592	0.698890
-38.966334	-2.052013	2.481766	0.007506	0.698949
-39.349110	-1.981591	2.491763	0.007577	0.698952
-39.023653	-1.993403	2.501760	0.007517	0.699045
-38.413278	-1.995886	2.511757	0.007404	0.699260
-38.128242	-2.047528	2.521754	0.007351	0.699258
-38.430996	-1.992532	2.531750	0.007408	0.699259
-37.710989	-1.969573	2.541747	0.007275	0.699566
-37.303122	-2.028684	2.551744	0.007199	0.699592
-37.500548	-1.992666	2.561741	0.007236	0.699593
-37.355864	-1.952902	2.571738	0.007210	0.699725
-36.596704	-2.007342	2.581734	0.007069	0.699889
-36.627702	-2.001082	2.591731	0.007075	0.699889
-36.433110	-2.029623	2.601728	0.007039	0.699901
-35.899428	-1.970740	2.611725	0.006940	0.700213
-35.421251	-2.056863	2.621722	0.006852	0.700210
-35.838094	-1.981370	2.631718	0.006930	0.700212
-35.385178	-1.977627	2.641715	0.006846	0.700382
-34.924993	-1.985721	2.651712	0.006761	0.700531
-35.127523	-1.951030	2.661709	0.006799	0.700528
-34.708739	-1.998687	2.671706	0.006721	0.700581
-34.020386	-1.979569	2.681702	0.006594	0.700868
-33.804048	-2.017145	2.691699	0.006554	0.700869
-33.897157	-1.999770	2.701696	0.006572	0.700870
-33.657081	-1.967554	2.711693	0.006527	0.701021
-33.075614	-2.024251	2.721690	0.006419	0.701115
-33.277767	-1.986698	2.731686	0.006458	0.701118
-32.934956	-2.015609	2.741683	0.006394	0.701182
-32.166326	-2.028857	2.751680	0.006251	0.701432
-32.369246	-1.994256	2.761677	0.006290	0.701428
-32.239066	-2.015964	2.771674	0.006266	0.701430
-31.830543	-1.976961	2.781670	0.006190	0.701656
-31.402526	-2.012889	2.791667	0.006111	0.701736
-31.352381	-2.021252	2.801664	0.006102	0.701737
-31.359167	-1.968288	2.811661	0.006104	0.701841
-30.310013	-2.045223	2.821658	0.005909	0.702063
-30.530338	-2.003079	2.831654	0.005950	0.702067
-30.490399	-2.010742	2.841651	0.005943	0.702066
-29.982087	-1.983084	2.851648	0.005849	0.702304
-29.753191	-1.994251	2.861645	0.005807	0.702363
-29.545458	-2.030597	2.871642	0.005769	0.702364
-29.641995	-1.947121	2.881638	0.005787	0.702497
-28.441297	-2.065891	2.891635	0.005564	0.702688
-28.743761	-2.012465	2.901632	0.005621	0.702686
-28.882151	-1.987057	2.911629	0.005647	0.702687
-28.294738	-1.955128	2.921626	0.005538	0.702962
-28.002854	-1.988329	2.931622	0.005484	0.703000
-27.828819	-2.019284	2.941619	0.005452	0.702999
-27.570037	-1.977387	2.951616	0.005404	0.703176
-26.974656	-2.005547	2.961613	0.005294	0.703332
-26.850710	-2.025403	2.971610	0.005271	0.703336
-27.116581	-1.977266	2.981606	0.005321	0.703337
-26.245871	-1.999311	2.991603	0.005160	0.703605
-26.270348	-1.982634	3.001600	0.005165	0.703629
-25.999412	-2.030632	3.011597	0.005115	0.703628
-26.039873	-1.962764	3.021594	0.005123	0.703750
-25.106809	-2.031685	3.031590	0.004949	0.703946
-25.095972	-2.031915	3.041587	0.004948	0.703948
-25.496060	-1.959850	3.051584	0.005023	0.703949
-24.433534	-2.010733	3.061581	0.004825	0.704227
-24.414673	-2.000492	3.071578	0.004822	0.704254
-24.311607	-2.016776	3.081574	0.004804	0.704257
-24.115686	-1.996734	3.091571	0.004767	0.704367
-23.504740	-1.994518	3.101568	0.004654	0.704590
-23.272782	-2.037464	3.111565	0.004611	0.704586
-23.473044	-2.003393	3.121562	0.004649	0.704582
-22.815444	-2.025868	3.131558	0.004527	0.704772
-22.382173	-2.047049	3.141555	0.004447	0.704884
-22.575328	-2.013587	3.151552	0.004483	0.704881
-22.630248	-1.984359	3.161549	0.004494	0.704920
-21.853438	-1.982192	3.171546	0.004350	0.705202
-21.634677	-2.019913	3.181542	0.004310	0.705204
-21.588462	-2.025749	3.191539	0.004301	0.705208
-21.229727	-1.989415	3.201536	0.004235	0.705409
-20.610774	-2.044418	3.211533	0.004120	0.705519
-20.957071	-1.982727	3.221530	0.004185	0.705518
-20.365393	-2.088091	3.231526	0.004075	0.705518
-20.031086	-1.986393	3.241523	0.004014	0.705841
-19.520114	-2.068392	3.251520	0.003919	0.705859
-19.709191	-2.035390	3.261517	0.003955	0.705857
-19.949113	-1.960643	3.271514	0.004000	0.705920
-19.106998	-2.010408	3.281510	0.003843	0.706121
-18.968788	-2.033922	3.291507	0.003818	0.706122
-19.205431	-1.990342	3.301504	0.003862	0.706124
-18.354510	-1.988912	3.311501	0.003704	0.706431
-18.458118	-1.967764	3.321498	0.003724	0.706436
-17.951389	-2.055296	3.331494	0.003630	0.706441
-17.963755	-1.959548	3.341491	0.003633	0.706628
-17.231886	-2.028773	3.351488	0.003497	0.706750
-17.436126	-1.993693	3.361485	0.003536	0.706746
-17.407034	-1.961101	3.371482	0.003531	0.706821
-16.156798	-2.055287	3.381478	0.003298	0.707079
-16.377143	-2.015937	3.391475	0.003340	0.707078
-16.414832	-2.009380	3.401472	0.003347	0.707077
-15.966648	-1.994079	3.411469	0.003264	0.707267
-15.628328	-2.002049	3.421466	0.003202	0.707371
-15.496997	-2.025813	3.431462	0.003178	0.707370
-15.444069	-2.010287	3.441459	0.003168	0.707419
-14.479580	-2.044729	3.451456	0.002989	0.707694
-14.394327	-2.059501	3.461453	0.002974	0.707694
-14.575029	-2.028466	3.471450	0.003008	0.707691
-14.387416	-2.007630	3.481446	0.002973	0.707799
-13.657662	-2.033874	3.491443	0.002838	0.708006
-13.665956	-2.031738	3.501440	0.002840	0.708006
-13.507463	-2.058940	3.511437	0.002811	0.708008
-12.984706	-2.030277	3.521434	0.002714	0.708251
-12.728336	-2.029295	3.531430	0.002667	0.708344
-12.617946	-2.046791	3.541427	0.002647	0.708347
-12.417968	-2.082478	3.551424	0.002610	0.708346
-12.226825	-1.982476	3.561421	0.002575	0.708614
-11.880843	-2.035015	3.571418	0.002511	0.708632
-11.708813	-2.062638	3.581414	0.002479	0.708637
-11.585770	-2.008830	3.591411	0.002457	0.708788
-10.731278	-2.080645	3.601408	0.002298	0.708948
-10.877208	-2.052886	3.611405	0.002326	0.708951
-10.800694	-2.064811	3.621402	0.002312	0.708953
-10.214063	-2.052120	3.631398	0.002203	0.709187
-10.092191	-2.035849	3.641395	0.002181	0.709262
-9.952266	-2.060284	3.651392	0.002155	0.709262
-10.148953	-1.991882	3.661389	0.002192	0.709328
-8.831284	-2.094835	3.671386	0.001947	0.709591
-8.977569	-2.065997	3.681382	0.001975	0.709596
-9.092949	-2.045518	3.691379	0.001997	0.709595
-8.580918	-2.074136	3.701376	0.001902	0.709719
-8.109462	-2.072408	3.711373	0.001815	0.709890
-8.033612	-2.087495	3.721370	0.001801	0.709886
-8.111608	-2.072742	3.731366	0.001816	0.709887
-7.580707	-2.058046	3.741363	0.001717	0.710104
-7.252223	-2.061530	3.751360	0.001657	0.710214
-7.469111	-2.022298	3.761357	0.001698	0.710214
-7.093431	-2.058787	3.771354	0.001628	0.710274
-6.275931	-2.075693	3.781350	0.001476	0.710530
-6.121597	-2.102499	3.791347	0.001448	0.710531
-6.286633	-2.072274	3.801344	0.001479	0.710532
-6.142687	-2.018572	3.811341	0.001453	0.710689
-5.122791	-2.111474	3.821338	0.001263	0.710866
-5.563214	-2.031001	3.831334	0.001346	0.710869
-5.261504	-2.083873	3.841331	0.001290	0.710870
-4.918972	-2.033135	3.851328	0.001227	0.711092
-4.694588	-2.052802	3.861325	0.001185	0.711132
-4.683892	-2.055028	3.871322	0.001184	0.711130
-4.285253	-2.056356	3.881318	0.001110	0.711269
-3.734250	-2.062839	3.891315	0.001008	0.711451
-3.793739	-2.051540	3.901312	0.001019	0.711451
-3.875367	-2.028852	3.911309	0.001035	0.711467
-2.855014	-2.064538	3.921306	0.000846	0.711757
-2.941582	-2.048728	3.931302	0.000862	0.711757
-2.798806	-2.071943	3.941299	0.000836	0.711761
-2.865166	-1.965762	3.951296	0.000849	0.711948
-2.291703	-1.998036	3.961293	0.000742	0.712086
-2.008858	-2.049031	3.971290	0.000690	0.712084
-2.043690	-1.995376	3.981286	0.000697	0.712178
-1.750844	-1.942982	3.991283	0.000643	0.712386
-1.397819	-2.005225	4.001280	0.000578	0.712386
-1.869392	-1.860703	4.011277	0.000666	0.712506
-1.305467	-1.861113	4.021274	0.000561	0.712704
-1.131170	-1.890057	4.031270	0.000529	0.712707
-1.134552	-1.770154	4.041267	0.000530	0.712944
-0.888930	-1.774069	4.051264	0.000485	0.713023
-1.127061	-1.666808	4.061261	0.000530	0.713151
-0.666242	-1.644154	4.071258	0.000444	0.713358
-0.824525	-1.581425	4.081254	0.000474	0.713426
-1.063863	-1.423568	4.091251	0.000519	0.713654
-0.587649	-1.439749	4.101248	0.000431	0.713790
-0.619402	-1.344221	4.111245	0.000437	0.713968
-0.494578	-1.266969	4.121242	0.000414	0.714165
-0.359081	-1.234631	4.131238	0.000390	0.714276
-0.407857	-1.064621	4.141235	0.000399	0.714596
-0.239984	-1.027467	4.151232	0.000368	0.714728
-0.276384	-0.933789	4.161229	0.000375	0.714900
-0.251343	-0.782264	4.171226	0.000371	0.715209
-0.307324	-0.671485	4.181222	0.000382	0.715408
-0.320590	-0.550118	4.191219	0.000385	0.715643
-0.071962	-0.470556	4.201216	0.000339	0.715888
-0.165596	-0.329861	4.211213	0.000356	0.716133
0.061184	-0.240008	4.221210	0.000315	0.716390
-0.077080	-0.086462	4.231206	0.000341	0.716644
-0.017457	0.048187	4.241203	0.000330	0.716931
0.000000	0.203795	4.251200	0.000327	0.717244
0.160632	0.803796	4.256205	0.000297	0.718486
0.172977	2.050692	4.261210	0.000294	0.720949
0.813914	3.788357	4.266214	0.000174	0.724584
1.015566	6.147528	4.271219	0.000135	0.729258
1.255907	9.021968	4.276224	0.000089	0.734912
1.620881	12.344362	4.281229	0.000019	0.741422
1.934094	16.122439	4.286234	-0.000042	0.748723
2.462143	20.289599	4.291238	-0.000143	0.756754
2.834727	24.856405	4.296243	-0.000215	0.765390
3.384443	29.777640	4.301248	-0.000320	0.774638
3.977139	35.032354	4.306253	-0.000434	0.784393
4.363878	40.651370	4.311258	-0.000509	0.794613
4.868780	46.546948	4.316262	-0.000607	0.805228
5.286145	52.744619	4.321267	-0.000688	0.816202
5.940445	59.160782	4.326272	-0.000814	0.827478
8.446057	65.520536	4.331277	-0.001285	0.839058
9.025918	72.439117	4.336282	-0.001397	0.850846
9.601975	79.572524	4.341286	-0.001509	0.862824
9.980973	86.928170	4.346291	-0.001584	0.874941
10.484675	94.418509	4.351296	-0.001682	0.887144
13.719571	101.612733	4.356301	-0.002289	0.899470
16.628729	109.070445	4.361306	-0.002835	0.911948
17.065612	117.090472	4.366310	-0.002922	0.924455
18.062255	125.119678	4.371315	-0.003112	0.936956
19.125716	133.250311	4.376320	-0.003315	0.949461
20.036715	141.491641	4.381325	-0.003490	0.961927
20.815710	149.834206	4.386330	-0.003640	0.974347
21.986028	158.194880	4.391334	-0.003864	0.986733
22.892569	166.657249	4.396339	-0.004038	0.999045
23.958637	175.113508	4.401344	-0.004241	1.011237
25.181717	183.602665	4.406349	-0.004474	1.023366
25.659787	192.251637	4.411354	-0.004569	1.035394
26.734923	200.820129	4.416358	-0.004774	1.047315
27.983913	209.395396	4.421363	-0.005012	1.059151
29.121261	218.027266	4.426368	-0.005230	1.070904
29.587706	226.764001	4.431373	-0.005322	1.082515
30.263125	235.460402	4.436378	-0.005453	1.093996
31.135113	244.121137	4.441382	-0.005621	1.105356
32.338590	252.733976	4.446387	-0.005850	1.116611
33.072739	261.407251	4.451392	-0.005992	1.127728
33.980749	270.070248	4.456397	-0.006167	1.138761
34.907071	278.725842	4.461402	-0.006345	1.149681
35.836888	287.383329	4.466406	-0.006523	1.160502
36.147864	296.095925	4.471411	-0.006587	1.171161
37.222424	304.670026	4.476416	-0.006792	1.181713
38.405996	313.236104	4.481421	-0.007018	1.192184
38.934371	321.874497	4.486426	-0.007122	1.202518
39.844453	330.460053	4.491430	-0.007297	1.212777
40.433608	339.072992	4.496435	-0.007412	1.222918
41.054934	347.688110	4.501440	-0.007533	1.232984
41.661669	356.262472	4.506445	-0.007651	1.242919
42.434922	364.789507	4.511450	-0.007800	1.252753
43.507364	373.267818	4.516454	-0.008005	1.262512
44.211137	381.803276	4.521459	-0.008142	1.272191
44.818460	390.315362	4.526464	-0.008260	1.281752
45.792996	398.770878	4.531469	-0.008447	1.291247
46.209356	407.294377	4.536474	-0.008530	1.300645
47.087024	415.797796	4.541478	-0.008699	1.310037
47.395313	424.383683	4.546483	-0.008761	1.319348
48.139414	432.774963	4.551488	-0.008905	1.328464
48.739878	441.213573	4.556493	-0.009022	1.337542
49.272378	449.617234	4.561498	-0.009127	1.346510
49.787654	458.059920	4.566502	-0.009228	1.355456
50.312962	466.440560	4.571507	-0.009331	1.364281
51.315289	474.760211	4.576512	-0.009523	1.373067
52.475176	483.049050	4.581517	-0.009744	1.381793
52.703605	491.497617	4.586522	-0.009792	1.390468
53.203609	499.893171	4.591526	-0.009890	1.399082
54.037536	508.196970	4.596531	-0.010051	1.407606
54.555303	516.570697	4.601536	-0.010152	1.416095
55.084373	524.914863	4.606541	-0.010256	1.424507
55.615423	533.271766	4.611546	-0.010360	1.432882
56.428567	541.559016	4.616550	-0.010517	1.441185
56.928664	549.881970	4.621555	-0.010615	1.449424
57.510964	558.201318	4.626560	-0.010729	1.457627
58.059843	566.505579	4.631565	-0.010836	1.465764
58.482573	574.871484	4.636570	-0.010920	1.473894
59.043951	583.153263	4.641574	-0.011030	1.481922
59.714878	591.402097	4.646579	-0.011160	1.489891
60.200523	599.695297	4.651584	-0.011255	1.497831
60.647694	607.971961	4.656589	-0.011344	1.505708
61.366081	616.217542	4.661594	-0.011483	1.513556
62.116471	624.445863	4.666598	-0.011627	1.521352
62.496153	632.733536	4.671603	-0.011703	1.529107
63.125243	640.985722	4.676608	-0.011826	1.536827
64.063886	649.180845	4.681613	-0.012006	1.544502
64.172953	657.515914	4.686618	-0.012031	1.552144
64.778594	665.745049	4.691622	-0.012149	1.559725
65.131030	673.993413	4.696627	-0.012220	1.567250
65.813892	682.209822	4.701632	-0.012352	1.574757
66.495502	690.414725	4.706637	-0.012484	1.582219
66.983546	698.645536	4.711642	-0.012580	1.589640
67.579274	706.882281	4.716646	-0.012696	1.597048
68.070227	715.095981	4.721651	-0.012793	1.604386
68.616860	723.315702	4.726656	-0.012900	1.611703
69.107033	731.550920	4.731661	-0.012996	1.618993
69.346602	739.783667	4.736666	-0.013046	1.626212
69.823310	748.061873	4.741670	-0.013140	1.633472
70.554156	756.209632	4.746675	-0.013281	1.640623
71.069967	764.381579	4.751680	-0.013382	1.647733
71.493136	772.602544	4.756685	-0.013466	1.654842
72.063082	780.763129	4.761690	-0.013577	1.661888
72.723150	788.939918	4.766694	-0.013705	1.668931
73.166296	797.143737	4.771699	-0.013793	1.675937
73.653601	805.313643	4.776704	-0.013889	1.682892
74.104097	813.512367	4.781709	-0.013978	1.689837
74.411688	821.722286	4.786714	-0.014040	1.696744
75.035563	829.876677	4.791718	-0.014161	1.703618
75.332573	838.091326	4.796723	-0.014222	1.710472
75.723871	846.277674	4.801728	-0.014300	1.717287
76.229209	854.438577	4.806733	-0.014399	1.724069
76.688529	862.593605	4.811738	-0.014490	1.730813
77.401886	870.736320	4.816742	-0.014627	1.737553
77.865188	878.893470	4.821747	-0.014719	1.744247
78.430082	887.048425	4.826752	-0.014829	1.750927
78.949594	895.225743	4.831757	-0.014931	1.757593
79.187148	903.406498	4.836762	-0.014980	1.764201
79.793572	911.557789	4.841766	-0.015098	1.770807
80.555878	919.682384	4.846771	-0.015245	1.777386
81.047732	927.842728	4.851776	-0.015342	1.783936
81.592849	936.030439	4.856781	-0.015449	1.790489
82.114893	944.212271	4.861786	-0.015551	1.797012
82.684346	952.324170	4.866790	-0.015662	1.803461
82.978976	960.492614	4.871795	-0.015722	1.809898
83.327027	968.643552	4.876800	-0.015792	1.816305
84.105490	976.734941	4.881805	-0.015942	1.822695
84.073463	984.941814	4.886810	-0.015941	1.829054
84.645988	993.079595	4.891814	-0.016053	1.835411
85.050460	1001.201710	4.896819	-0.016133	1.841713
85.364619	1009.348385	4.901824	-0.016197	1.848002
85.720260	1017.516363	4.906829	-0.016268	1.854290
86.389440	1025.597357	4.911834	-0.016398	1.860528
87.006796	1033.722262	4.916838	-0.016518	1.866771
87.255322	1041.913707	4.921843	-0.016569	1.873002
87.692312	1050.030391	4.926848	-0.016656	1.879177
88.176118	1058.150849	4.931853	-0.016751	1.885340
88.610461	1066.267900	4.936858	-0.016837	1.891474
88.926869	1074.428788	4.941862	-0.016901	1.897608
89.178165	1082.560560	4.946867	-0.016952	1.903693
89.718508	1090.660074	4.951872	-0.017058	1.909767
90.298110	1098.778246	4.956877	-0.017171	1.915839
90.804334	1106.869368	4.961882	-0.017270	1.921865
91.145930	1115.008209	4.966886	-0.017339	1.927888
91.946360	1123.099637	4.971891	-0.017493	1.933908
92.383890	1131.221117	4.976896	-0.017580	1.939891
93.299385	1139.294957	4.981901	-0.017755	1.945874
93.784547	1147.462053	4.986906	-0.017851	1.951858
94.113320	1155.619583	4.991910	-0.017917	1.957801
94.458599	1163.729778	4.996915	-0.017986	1.963692
94.946851	1171.815035	5.001920	-0.018082	1.969564
95.513546	1179.939939	5.006925	-0.018193	1.975455
95.624858	1188.066149	5.011930	-0.018219	1.981280
96.028620	1196.179421	5.016934	-0.018299	1.987110
96.317436	1204.317486	5.021939	-0.018358	1.992929
96.582208	1212.418355	5.026944	-0.018412	1.998701
97.571218	1220.427960	5.031949	-0.018601	2.004469
97.937330	1228.555495	5.036954	-0.018675	2.010237
98.404284	1236.673994	5.041958	-0.018767	2.015993
98.840693	1244.780917	5.046963	-0.018853	2.021722
99.023176	1252.915123	5.051968	-0.018892	2.027426
99.503057	1261.047657	5.056973	-0.018986	2.033145
99.584855	1269.181552	5.061978	-0.019007	2.038807
100.227634	1277.226633	5.066982	-0.019131	2.044449
100.665508	1285.322953	5.071987	-0.019218	2.050090
100.988559	1293.444028	5.076992	-0.019283	2.055721
101.721134	1301.498160	5.081997	-0.019425	2.061331
102.027674	1309.600614	5.087002	-0.019487	2.066917
102.578074	1317.708404	5.092006	-0.019594	2.072515
102.883697	1325.807078	5.097011	-0.019656	2.078068
103.126187	1333.909738	5.102016	-0.019707	2.083602
103.555094	1342.022954	5.107021	-0.019791	2.089147
103.573779	1350.170252	5.112026	-0.019800	2.094660
104.058374	1358.233980	5.117030	-0.019895	2.100148
104.615432	1366.307307	5.122035	-0.020004	2.105634
104.897972	1374.445783	5.127040	-0.020062	2.111124
105.386850	1382.573088	5.132045	-0.020158	2.116611
105.773095	1390.614472	5.137050	-0.020235	2.122017
106.200113	1398.694742	5.142054	-0.020319	2.127439
106.751611	1406.769599	5.147059	-0.020427	2.132856
107.217031	1414.845694	5.152064	-0.020519	2.138251
107.517107	1422.955382	5.157069	-0.020580	2.143639
107.530482	1431.076030	5.162074	-0.020587	2.148993
107.949582	1439.172967	5.167078	-0.020670	2.154357
108.703252	1447.179022	5.172083	-0.020816	2.159679
108.917228	1455.265877	5.177088	-0.020861	2.164991
109.471966	1463.337890	5.182093	-0.020969	2.170311
109.576248	1471.477629	5.187098	-0.020993	2.175620
109.870596	1479.558140	5.192102	-0.021053	2.180896
110.262742	1487.633484	5.197107	-0.021131	2.186164
110.720840	1495.720481	5.202112	-0.021222	2.191433
111.302829	1503.798624	5.207117	-0.021335	2.196695
111.503019	1511.879795	5.212122	-0.021377	2.201912
112.002032	1519.944481	5.217126	-0.021475	2.207132
112.586761	1528.006803	5.222131	-0.021589	2.212347
112.737100	1536.109054	5.227136	-0.021622	2.217535
113.045821	1544.200068	5.232141	-0.021685	2.222719
113.331874	1552.285360	5.237146	-0.021743	2.227884
113.665378	1560.389643	5.242150	-0.021810	2.233054
113.856844	1568.491331	5.247155	-0.021851	2.238197
114.211902	1576.524849	5.252160	-0.021922	2.243300
114.611880	1584.604155	5.257165	-0.022002	2.248425
114.955339	1592.689917	5.262170	-0.022071	2.253536
115.509184	1600.723167	5.267174	-0.022179	2.258621
116.111222	1608.770981	5.272179	-0.022296	2.263708
116.408731	1616.861787	5.277184	-0.022356	2.268784
116.807497	1625.042229	5.282189	-0.022436	2.273913
117.142438	1633.080253	5.287194	-0.022503	2.278937
117.431232	1641.140361	5.292198	-0.022562	2.283959
117.636408	1649.222878	5.297203	-0.022605	2.288976
118.085110	1657.286719	5.302208	-0.022694	2.293992
118.475229	1665.347918	5.307213	-0.022771	2.298990
118.650404	1673.416531	5.312218	-0.022809	2.303964
118.931311	1681.499428	5.317222	-0.022866	2.308945
119.420899	1689.579077	5.322227	-0.022963	2.313930
119.767414	1697.620562	5.327232	-0.023032	2.318869
120.163145	1705.680160	5.332237	-0.023111	2.323813
120.434797	1713.753811	5.337242	-0.023167	2.328744
120.922885	1721.824328	5.342246	-0.023262	2.333681
121.146070	1729.911117	5.347251	-0.023309	2.338595
121.318134	1737.977789	5.352256	-0.023346	2.343483
121.731926	1746.049403	5.357261	-0.023428	2.348383
121.876767	1754.165734	5.362266	-0.023460	2.353278
122.315395	1762.203414	5.367270	-0.023547	2.358139
122.793884	1770.237742	5.372275	-0.023641	2.362991
123.165053	1778.280638	5.377280	-0.023715	2.367830
123.517489	1786.372620	5.382285	-0.023786	2.372687
123.837608	1794.436960	5.387290	-0.023851	2.377514
124.261802	1802.483970	5.392294	-0.023935	2.382330
124.434270	1810.575476	5.397299	-0.023972	2.387142
124.842931	1818.642338	5.402304	-0.024053	2.391949
125.240643	1826.716060	5.407309	-0.024132	2.396749
125.471330	1834.768342	5.412314	-0.024180	2.401514
125.745681	1842.826978	5.417318	-0.024236	2.406276
126.233113	1850.893928	5.422323	-0.024332	2.411050
126.523807	1858.964921	5.427328	-0.024391	2.415802
126.942289	1867.017696	5.432333	-0.024474	2.420544
127.276590	1875.064760	5.437338	-0.024541	2.425266
127.752587	1883.137170	5.442342	-0.024635	2.430005
128.396105	1891.259451	5.447347	-0.024760	2.434777
128.400165	1899.316758	5.452352	-0.024766	2.439452
128.820989	1907.351686	5.457357	-0.024849	2.444137
129.124633	1915.392570	5.462362	-0.024910	2.448808
129.368108	1923.479385	5.467366	-0.024961	2.453491
129.502100	1931.551660	5.472371	-0.024991	2.458149
129.865408	1939.585690	5.477376	-0.025063	2.462794
130.210871	1947.650806	5.482381	-0.025133	2.467446
131.111160	1955.664194	5.487386	-0.025305	2.472101
131.910457	1963.699316	5.492390	-0.025459	2.476752
132.496401	1971.751506	5.497395	-0.025573	2.481388
132.687292	1979.809772	5.502400	-0.025614	2.485990
133.020258	1987.912525	5.507405	-0.025681	2.490618
133.307755	1995.985770	5.512410	-0.025740	2.495218
133.692220	2004.011892	5.517414	-0.025816	2.499790
134.049397	2012.064775	5.522419	-0.025888	2.504367
134.421952	2020.121776	5.527424	-0.025962	2.508938
134.868961	2028.227706	5.532429	-0.026050	2.513534
134.995652	2036.297330	5.537434	-0.026079	2.518078
135.536372	2044.298712	5.542438	-0.026185	2.522606
135.802076	2052.374588	5.547443	-0.026239	2.527147
135.855933	2060.452563	5.552448	-0.026254	2.531666
136.476452	2068.491423	5.557453	-0.026375	2.536195
136.521275	2076.560651	5.562458	-0.026388	2.540692
136.929445	2084.591781	5.567462	-0.026469	2.545186
137.300795	2092.659780	5.572467	-0.026544	2.549690
137.676493	2100.720579	5.577472	-0.026618	2.554182
137.832694	2108.806102	5.582477	-0.026653	2.558664
138.061928	2116.830160	5.587482	-0.026700	2.563110
138.519544	2124.851074	5.592486	-0.026791	2.567562
138.810262	2132.947007	5.597491	-0.026850	2.572035
138.983032	2141.010337	5.602496	-0.026887	2.576475
139.397795	2149.058977	5.607501	-0.026969	2.580916
139.535972	2157.099363	5.612506	-0.027000	2.585326
139.946301	2165.146054	5.617510	-0.027081	2.589750
140.585677	2173.366598	5.622515	-0.027206	2.594277
140.820750	2181.361429	5.627520	-0.027254	2.598646
141.273778	2189.360784	5.632525	-0.027344	2.603024
141.422684	2197.382108	5.637530	-0.027376	2.607387
141.872630	2205.416445	5.642534	-0.027465	2.611769
141.924308	2213.518047	5.647539	-0.027480	2.616153
142.202487	2221.536328	5.652544	-0.027537	2.620501
142.555575	2229.559987	5.657549	-0.027607	2.624849
142.912589	2237.599877	5.662554	-0.027679	2.629199
143.172319	2245.664723	5.667558	-0.027732	2.633548
143.493670	2253.713917	5.672563	-0.027797	2.637886
143.785005	2261.734730	5.677568	-0.027856	2.642199
144.140137	2269.803086	5.682573	-0.027928	2.646535
144.506042	2277.839951	5.687578	-0.028001	2.650848
144.792882	2285.906256	5.692582	-0.028059	2.655164
145.269807	2293.934440	5.697587	-0.028153	2.659465
145.378250	2301.985564	5.702592	-0.028178	2.663748
145.830270	2310.048528	5.707597	-0.028267	2.668052
146.002922	2318.119212	5.712602	-0.028305	2.672335
146.186343	2326.193369	5.717606	-0.028344	2.676614
146.421503	2334.231060	5.722611	-0.028393	2.680870
146.732601	2342.215538	5.727616	-0.028455	2.685096
147.302303	2350.252228	5.732621	-0.028567	2.689359
147.367378	2358.343847	5.737626	-0.028584	2.693612
147.628638	2366.390703	5.742630	-0.028637	2.697847
147.960179	2374.421618	5.747635	-0.028704	2.702072
148.299384	2382.444654	5.752640	-0.028772	2.706286
148.724206	2390.504866	5.757645	-0.028856	2.710519
149.187768	2398.544509	5.762650	-0.028948	2.714736
149.365381	2406.608867	5.767654	-0.028986	2.718942
149.684354	2414.637681	5.772659	-0.029050	2.723132
150.082258	2422.656397	5.777664	-0.029129	2.727315
150.400549	2430.760484	5.782669	-0.029194	2.731530
150.428074	2438.824157	5.787674	-0.029204	2.735701
150.840097	2446.835837	5.792678	-0.029286	2.739861
151.265150	2454.867490	5.797683	-0.029370	2.744027
151.381397	2462.931066	5.802688	-0.029396	2.748183
151.781745	2471.029977	5.807693	-0.029476	2.752369
152.012416	2479.122450	5.812698	-0.029524	2.756535
152.217254	2487.118118	5.817702	-0.029567	2.760643
152.732949	2495.098514	5.822707	-0.029668	2.764756
152.844222	2503.138455	5.827712	-0.029694	2.768869
153.259930	2511.197712	5.832717	-0.029776	2.773004
153.715736	2519.208112	5.837722	-0.029866	2.777110
154.020445	2527.251312	5.842726	-0.029928	2.781217
154.483619	2535.304762	5.847731	-0.030019	2.785333
154.490727	2543.367276	5.852736	-0.030026	2.789421
154.993107	2551.424324	5.857741	-0.030124	2.793529
155.455531	2559.448697	5.862746	-0.030215	2.797612
155.594875	2567.496392	5.867750	-0.030246	2.801682
155.963561	2575.531898	5.872755	-0.030320	2.805753
156.415076	2583.529396	5.877760	-0.030409	2.809804
156.705115	2591.636217	5.882765	-0.030468	2.813894
156.647093	2599.706536	5.887770	-0.030462	2.817940
156.964561	2607.746031	5.892774	-0.030526	2.821987
157.254198	2615.791690	5.897779	-0.030585	2.826029
157.279745	2623.825413	5.902784	-0.030595	2.830044
157.641561	2631.908007	5.907789	-0.030668	2.834097
157.897603	2639.925993	5.912794	-0.030720	2.838106
158.222616	2647.939465	5.917798	-0.030786	2.842111
158.677462	2655.950960	5.922803	-0.030875	2.846116
158.878777	2663.964914	5.927808	-0.030918	2.850103
159.485835	2672.021294	5.932813	-0.031036	2.854128
160.020355	2680.042626	5.937818	-0.031141	2.858126
160.311354	2688.095957	5.942822	-0.031200	2.862120
160.850402	2696.114452	5.947827	-0.031305	2.866105
161.019742	2704.162434	5.952832	-0.031342	2.870079
161.351295	2712.260657	5.957837	-0.031408	2.874081
161.681726	2720.275717	5.962842	-0.031475	2.878036
162.103594	2728.285413	5.967846	-0.031559	2.881988
162.342835	2736.339447	5.972851	-0.031608	2.885946
162.419543	2744.389549	5.977856	-0.031627	2.889889
162.992356	2752.458270	5.982861	-0.031739	2.893861
162.940242	2760.528267	5.987866	-0.031734	2.897795
163.191820	2768.553157	5.992870	-0.031786	2.901719
163.532050	2776.571552	5.997875	-0.031855	2.905638
163.919360	2784.593200	6.002880	-0.031932	2.909556
164.048753	2792.736684	6.007885	-0.031961	2.913514
164.312132	2800.754738	6.012890	-0.032015	2.917413
164.539911	2808.756582	6.017894	-0.032062	2.921297
164.806447	2816.781769	6.022899	-0.032117	2.925189
164.985529	2824.796928	6.027904	-0.032155	2.929067
165.492827	2832.837561	6.032909	-0.032255	2.932969
165.827915	2840.872886	6.037914	-0.032322	2.936854
165.915578	2848.899139	6.042918	-0.032344	2.940716
166.199891	2856.946547	6.047923	-0.032402	2.944594
166.309739	2864.992992	6.052928	-0.032427	2.948457
166.667264	2873.040242	6.057933	-0.032499	2.952329
166.807391	2881.107340	6.062938	-0.032530	2.956193
167.133505	2889.079335	6.067942	-0.032595	2.960017
167.208775	2897.120891	6.072947	-0.032614	2.963855
167.513088	2905.165387	6.077952	-0.032676	2.967702
167.751389	2913.222308	6.082957	-0.032726	2.971547
168.038506	2921.269449	6.087962	-0.032784	2.975384
168.166580	2929.280902	6.092966	-0.032813	2.979191
168.705776	2937.332052	6.097971	-0.032918	2.983033
168.974703	2945.355283	6.102976	-0.032973	2.986843
169.222973	2953.412253	6.107981	-0.033025	2.990663
169.478328	2961.480897	6.112986	-0.033077	2.994484
169.757731	2969.493823	6.117990	-0.033134	2.998276
170.167227	2977.497998	6.122995	-0.033216	3.002064
170.374409	2985.508579	6.128000	-0.033259	3.005841
170.776204	2993.534823	6.133005	-0.033339	3.009630
170.825620	3001.631711	6.138010	-0.033353	3.013429
170.786744	3009.692083	6.143014	-0.033351	3.017203
171.339256	3017.711351	6.148019	-0.033459	3.020982
171.384122	3025.708378	6.153024	-0.033472	3.024720
171.708933	3033.771840	6.158029	-0.033538	3.028499
171.829624	3041.819193	6.163034	-0.033565	3.032255
172.256834	3049.844768	6.168038	-0.033650	3.036011
172.602276	3057.837245	6.173043	-0.033719	3.039744
172.747752	3065.880599	6.178048	-0.033751	3.043486
173.015925	3073.924632	6.183053	-0.033806	3.047229
173.129385	3081.979809	6.188058	-0.033832	3.050965
173.416726	3090.018937	6.193062	-0.033891	3.054698
173.718189	3098.050376	6.198067	-0.033952	3.058423
174.192370	3106.050380	6.203072	-0.034045	3.062137
174.544354	3114.093856	6.208077	-0.034116	3.065861
174.563199	3122.141267	6.213082	-0.034124	3.069567
174.870109	3130.266906	6.218086	-0.034187	3.073317
175.183396	3138.295870	6.223091	-0.034250	3.077019
175.322609	3146.268566	6.228096	-0.034281	3.080682
175.734015	3154.239622	6.233101	-0.034362	3.084353
175.964566	3162.295339	6.238106	-0.034410	3.088050
176.225529	3170.337259	6.243110	-0.034464	3.091737
176.605082	3178.396822	6.248115	-0.034540	3.095434
176.851930	3186.395970	6.253120	-0.034591	3.099092
177.142493	3194.435300	6.258125	-0.034650	3.102766
177.348524	3202.475609	6.263130	-0.034693	3.106433
177.509932	3210.506609	6.268134	-0.034728	3.110089
177.803222	3218.567726	6.273139	-0.034788	3.113760
177.847364	3226.595767	6.278144	-0.034801	3.117401
178.337856	3234.606132	6.283149	-0.034897	3.121049
178.767133	3242.583834	6.288154	-0.034982	3.124675
179.004091	3250.650232	6.293158	-0.035031	3.128329
179.248895	3258.739261	6.298163	-0.035082	3.131989
179.455894	3266.768815	6.303168	-0.035126	3.135616
179.562559	3274.800294	6.308173	-0.035150	3.139235
179.673867	3282.822579	6.313178	-0.035176	3.142847
180.294991	3290.834815	6.318182	-0.035297	3.146472
180.851049	3298.866455	6.323187	-0.035405	3.150098
180.771265	3306.945278	6.328192	-0.035396	3.153714
181.099361	3314.957315	6.333197	-0.035462	3.157313
181.395331	3322.982486	6.338202	-0.035522	3.160913
181.603219	3330.975126	6.343206	-0.035566	3.164490
181.828504	3339.019366	6.348211	-0.035612	3.168087
182.077564	3347.056545	6.353216	-0.035664	3.171677
182.633353	3355.082518	6.358221	-0.035772	3.175272
182.722747	3363.134629	6.363226	-0.035794	3.178854
182.964497	3371.153096	6.368230	-0.035844	3.182424
183.150378	3379.194500	6.373235	-0.035884	3.185997
183.245329	3387.226927	6.378240	-0.035906	3.189559
183.530706	3395.288340	6.383245	-0.035965	3.193137
184.037553	3403.300387	6.388250	-0.036064	3.196699
184.242101	3411.311439	6.393254	-0.036107	3.200244
184.305732	3419.344139	6.398259	-0.036124	3.203789
184.539346	3427.359043	6.403264	-0.036172	3.207328
184.793902	3435.431358	6.408269	-0.036225	3.210890
184.811479	3443.463315	6.413274	-0.036233	3.214421
185.089468	3451.491005	6.418278	-0.036290	3.217956
185.486114	3459.513678	6.423283	-0.036369	3.221490
185.740532	3467.498067	6.428288	-0.036421	3.224998
185.937132	3475.579505	6.433293	-0.036463	3.228541
186.310976	3483.634807	6.438298	-0.036537	3.232077
186.379871	3491.693880	6.443302	-0.036555	3.235598
186.671808	3499.700221	6.448307	-0.036615	3.239101
186.933220	3507.662276	6.453312	-0.036668	3.242580
187.388029	3515.695524	6.458317	-0.036758	3.246094
187.692626	3523.733608	6.463322	-0.036820	3.249600
187.792827	3531.792882	6.468326	-0.036843	3.253103
187.862712	3539.846402	6.473331	-0.036861	3.256599
188.000115	3547.834649	6.478336	-0.036892	3.260065
188.142345	3555.880831	6.483341	-0.036923	3.263553
188.429295	3563.900801	6.488346	-0.036982	3.267032
188.881991	3571.894105	6.493350	-0.037071	3.270501
189.004443	3579.988432	6.498355	-0.037099	3.273998
189.299076	3587.980171	6.503360	-0.037159	3.277453
189.632189	3596.011113	6.508365	-0.037226	3.280924
189.876295	3603.996299	6.513370	-0.037276	3.284367
189.935737	3612.039363	6.518374	-0.037292	3.287824
190.241851	3620.108042	6.523379	-0.037354	3.291298
190.636675	3628.123512	6.528384	-0.037433	3.294749
190.802553	3636.176119	6.533389	-0.037469	3.298204
191.132487	3644.183158	6.538394	-0.037535	3.301641
191.367474	3652.176473	6.543398	-0.037584	3.305066
191.608608	3660.258878	6.548403	-0.037634	3.308525
191.930664	3668.293599	6.553408	-0.037699	3.311963
192.252056	3676.323690	6.558413	-0.037764	3.315396
192.253287	3684.339921	6.563418	-0.037769	3.318807
192.457686	3692.352361	6.568422	-0.037812	3.322221
192.709328	3700.377815	6.573427	-0.037864	3.325638
192.814636	3708.400205	6.578432	-0.037889	3.329045
192.995161	3716.444917	6.583437	-0.037927	3.332461
193.311017	3724.484667	6.588442	-0.037991	3.335876
193.499859	3732.495885	6.593446	-0.038031	3.339271
193.807717	3740.530130	6.598451	-0.038094	3.342676
193.733956	3748.587366	6.603456	-0.038085	3.346074
194.134300	3756.590189	6.608461	-0.038164	3.349463
194.304640	3764.644194	6.613466	-0.038201	3.352861
194.321744	3772.702602	6.618470	-0.038209	3.356252
194.796169	3780.685221	6.623475	-0.038303	3.359625
195.083379	3788.657209	6.628480	-0.038361	3.362982
195.314514	3796.721788	6.633485	-0.038409	3.366373
195.708416	3804.750140	6.638490	-0.038488	3.369752
195.938442	3812.809674	6.643494	-0.038535	3.373134
196.339532	3820.809079	6.648499	-0.038615	3.376493
196.445790	3828.818502	6.653504	-0.038640	3.379843
197.017393	3836.839916	6.658509	-0.038751	3.383211
197.121783	3844.903844	6.663514	-0.038776	3.386577
197.257438	3852.919971	6.668518	-0.038806	3.389921
197.571529	3861.052179	6.673523	-0.038870	3.393316
197.786016	3869.056777	6.678528	-0.038915	3.396651
198.181276	3877.030143	6.683533	-0.038993	3.399975
198.619963	3885.002610	6.688538	-0.039080	3.403298
198.635539	3893.022112	6.693542	-0.039088	3.406623
198.871959	3901.059009	6.698547	-0.039137	3.409958
199.056261	3909.121055	6.703552	-0.039176	3.413300
199.386219	3917.151073	6.708557	-0.039243	3.416629
199.826772	3925.140612	6.713562	-0.039330	3.419943
199.874966	3933.152254	6.718566	-0.039344	3.423248
200.070340	3941.217189	6.723571	-0.039385	3.426578
200.292186	3949.263615	6.728576	-0.039431	3.429898
200.467412	3957.291377	6.733581	-0.039469	3.433205
200.767385	3965.322113	6.738586	-0.039530	3.436514
200.981171	3973.306109	6.743590	-0.039575	3.439798
201.260567	3981.335933	6.748595	-0.039632	3.443100
201.272190	3989.380806	6.753600	-0.039639	3.446396
201.593459	3997.378604	6.758605	-0.039704	3.449680
201.923462	4005.456051	6.763610	-0.039770	3.452993
202.071221	4013.475780	6.768614	-0.039803	3.456274
202.483734	4021.493446	6.773619	-0.039884	3.459559
202.552155	4029.523485	6.778624	-0.039902	3.462835
202.916276	4037.553663	6.783629	-0.039975	3.466117
203.137207	4045.580773	6.788634	-0.040021	3.469391
203.184551	4053.640888	6.793638	-0.040035	3.472669
203.636272	4061.658144	6.798643	-0.040124	3.475939
203.813727	4069.621711	6.803648	-0.040162	3.479176
204.322233	4077.631399	6.808653	-0.040262	3.482439
204.715093	4085.676450	6.813658	-0.040340	3.485710
204.619632	4093.713525	6.818662	-0.040327	3.488959
205.079969	4101.757820	6.823667	-0.040418	3.492225
205.271486	4109.764340	6.828672	-0.040459	3.495464
205.643445	4117.782135	6.833677	-0.040533	3.498711
205.950929	4125.814889	6.838682	-0.040595	3.501959
206.042012	4133.814622	6.843686	-0.040617	3.505183
206.457923	4141.853333	6.848691	-0.040700	3.508430
206.519122	4149.910721	6.853696	-0.040716	3.511671
206.835803	4157.939606	6.858701	-0.040780	3.514905
207.198146	4165.946066	6.863706	-0.040852	3.518128
207.517910	4173.954729	6.868710	-0.040917	3.521348
207.646700	4181.967513	6.873715	-0.040946	3.524561
207.957531	4190.005822	6.878720	-0.041009	3.527787
208.009911	4198.045477	6.883725	-0.041024	3.531002
208.118767	4206.117150	6.888730	-0.041049	3.534229
208.405659	4214.116271	6.893734	-0.041107	3.537429
208.862154	4222.124097	6.898739	-0.041197	3.540635
208.940882	4230.143476	6.903744	-0.041217	3.543832
209.174844	4238.182835	6.908749	-0.041266	3.547038
209.329472	4246.238654	6.913754	-0.041299	3.550245
209.511824	4254.322573	6.918758	-0.041338	3.553461
209.722947	4262.393663	6.923763	-0.041383	3.556670
210.047164	4270.297535	6.928768	-0.041448	3.559814
210.189884	4278.338668	6.933773	-0.041480	3.563003
210.281174	4286.361673	6.938778	-0.041502	3.566181
210.510259	4294.327238	6.943782	-0.041549	3.569337
211.078904	4302.377821	6.948787	-0.041660	3.572534
211.091635	4310.428304	6.953792	-0.041668	3.575712
211.484741	4318.436806	6.958797	-0.041746	3.578882
211.507752	4326.469234	6.963802	-0.041755	3.582047
211.725060	4334.446275	6.968806	-0.041800	3.585193
212.086255	4342.496246	6.973811	-0.041873	3.588370
212.097331	4350.547808	6.978816	-0.041880	3.591534
212.190633	4358.557600	6.983821	-0.041902	3.594681
212.351747	4366.579143	6.988826	-0.041937	3.597832
212.842057	4374.551539	6.993830	-0.042033	3.600970
213.034315	4382.585914	6.998835	-0.042074	3.604122
212.803860	4390.628793	7.003840	-0.042036	3.607262
213.166192	4398.646048	7.008845	-0.042109	3.610406
213.647398	4406.674835	7.013850	-0.042203	3.613555
213.885888	4414.692780	7.018854	-0.042253	3.616690
213.978055	4422.727308	7.023859	-0.042275	3.619824
214.207992	4430.730299	7.028864	-0.042323	3.622948
214.454348	4438.757614	7.033869	-0.042374	3.626079
214.309826	4446.848220	7.038874	-0.042352	3.629221
214.522695	4454.873438	7.043878	-0.042397	3.632344
214.795419	4462.915989	7.048883	-0.042452	3.635473
214.867337	4470.897372	7.053888	-0.042471	3.638571
215.167174	4478.918204	7.058893	-0.042532	3.641687
215.640090	4486.897816	7.063898	-0.042625	3.644789
215.967205	4494.924339	7.068902	-0.042690	3.647902
216.123331	4503.001106	7.073907	-0.042725	3.651028
216.449277	4511.028784	7.078912	-0.042790	3.654137
216.825582	4519.035734	7.083917	-0.042865	3.657236
217.035149	4527.035052	7.088922	-0.042909	3.660325
217.162039	4535.051694	7.093926	-0.042938	3.663416
217.498286	4543.134071	7.098931	-0.043006	3.666536
217.443288	4551.122312	7.103936	-0.043000	3.669606
217.610200	4559.182804	7.108941	-0.043037	3.672707
217.932531	4567.206424	7.113946	-0.043102	3.675795
218.271638	4575.160088	7.118950	-0.043170	3.678854
218.401157	4583.252661	7.123955	-0.043199	3.681959
218.701985	4591.211059	7.128960	-0.043260	3.685014
218.820237	4599.240534	7.133965	-0.043287	3.688089
218.938796	4607.283285	7.138970	-0.043314	3.691166
218.928709	4615.299566	7.143974	-0.043317	3.694227
219.516998	4623.355268	7.148979	-0.043432	3.697316
219.463670	4631.349358	7.153984	-0.043427	3.700363
219.762732	4639.355732	7.158989	-0.043487	3.703421
220.157973	4647.368353	7.163994	-0.043566	3.706481
220.403701	4655.391721	7.168998	-0.043617	3.709538
220.525204	4663.532584	7.174003	-0.043644	3.712635
220.709526	4671.555344	7.179008	-0.043684	3.715686
221.061536	4679.490045	7.184013	-0.043754	3.718705
221.158127	4687.555643	7.189018	-0.043777	3.721765
220.950704	4695.503863	7.194022	-0.043744	3.724770
221.402584	4703.569121	7.199027	-0.043833	3.727834
221.455270	4711.569917	7.204032	-0.043848	3.730860
221.563915	4719.623297	7.209037	-0.043873	3.733906
221.932496	4727.662776	7.214042	-0.043946	3.736950
222.009288	4735.598993	7.219046	-0.043966	3.739945
222.291326	4743.671270	7.224051	-0.044023	3.742995
222.439833	4751.660747	7.229056	-0.044056	3.746007
222.726484	4759.691281	7.234061	-0.044114	3.749036
222.892437	4767.789928	7.239066	-0.044150	3.752085
222.866866	4775.791543	7.244070	-0.044150	3.755090
223.280996	4783.811537	7.249075	-0.044233	3.758110
223.608916	4791.825155	7.254080	-0.044299	3.761124
223.921046	4799.802984	7.259085	-0.044362	3.764121
224.104473	4807.826873	7.264090	-0.044401	3.767130
224.524733	4815.831986	7.269094	-0.044484	3.770135
224.668085	4823.913119	7.274099	-0.044516	3.773159
224.733178	4831.931972	7.279104	-0.044533	3.776157
225.090425	4839.938767	7.284109	-0.044605	3.779153
225.152108	4847.974043	7.289114	-0.044621	3.782152
225.060928	4855.985505	7.294118	-0.044609	3.785135
225.467130	4864.006244	7.299123	-0.044690	3.788131
225.649806	4872.042632	7.304128	-0.044729	3.791126
225.678423	4880.112247	7.309133	-0.044739	3.794126
226.068345	4888.113928	7.314138	-0.044817	3.797108
226.185755	4896.084297	7.319142	-0.044844	3.800069
226.603078	4904.101412	7.324147	-0.044926	3.803052
226.445304	4912.138476	7.329152	-0.044902	3.806027
226.813193	4920.124930	7.334157	-0.044975	3.808993
227.162809	4928.204928	7.339162	-0.045046	3.811990
227.310304	4936.173086	7.344166	-0.045078	3.814939
227.723098	4944.211608	7.349171	-0.045160	3.817918
227.973992	4952.218544	7.354176	-0.045212	3.820879
228.035163	4960.224073	7.359181	-0.045228	3.823834
228.120477	4968.285284	7.364186	-0.045249	3.826807
228.298823	4976.278816	7.369190	-0.045287	3.829754
228.528981	4984.349478	7.374195	-0.045335	3.832729
228.579261	4992.360267	7.379200	-0.045349	3.835676
228.919880	5000.368508	7.384205	-0.045418	3.838626
229.149635	5008.412265	7.389210	-0.045466	3.841584
229.044090	5016.377264	7.394214	-0.045451	3.844504
229.519941	5024.424002	7.399219	-0.045544	3.847464
229.572637	5032.433346	7.404224	-0.045559	3.850399
229.703386	5040.477778	7.409229	-0.045589	3.853346
230.056001	5048.539226	7.414234	-0.045659	3.856301
230.131679	5056.531685	7.419238	-0.045678	3.859224
230.525222	5064.553848	7.424243	-0.045757	3.862161
230.434163	5072.542037	7.429248	-0.045745	3.865075
230.527692	5080.628945	7.434253	-0.045767	3.868025
230.945426	5088.633325	7.439258	-0.045850	3.870950
231.126717	5096.855758	7.444262	-0.045889	3.873947
231.569488	5104.862791	7.449267	-0.045976	3.876869
231.776604	5112.742661	7.454272	-0.046020	3.879737
231.754032	5120.737045	7.459277	-0.046021	3.882641
232.066775	5128.700601	7.464282	-0.046084	3.885537
232.264426	5136.732325	7.469286	-0.046126	3.888454
232.356434	5144.797307	7.474291	-0.046148	3.891379
232.352841	5152.773407	7.479296	-0.046152	3.894267
232.749634	5160.810344	7.484301	-0.046231	3.897183
233.286445	5168.805554	7.489306	-0.046336	3.900084
233.422973	5176.830423	7.494310	-0.046366	3.902987
233.673940	5184.846734	7.499315	-0.046418	3.905886
233.924260	5192.860493	7.504320	-0.046470	3.908782
233.965744	5200.914467	7.509325	-0.046482	3.911686
234.244087	5208.945812	7.514330	-0.046539	3.914585
234.161795	5216.959180	7.519334	-0.046529	3.917468
234.666817	5224.964977	7.524339	-0.046628	3.920357
234.842247	5232.960624	7.529344	-0.046666	3.923234
234.869062	5240.954090	7.534349	-0.046676	3.926106
235.342095	5248.990107	7.539354	-0.046769	3.928999
235.399778	5257.033950	7.544358	-0.046784	3.931885
235.358251	5265.092181	7.549363	-0.046782	3.934772
235.673461	5273.099307	7.554368	-0.046845	3.937645
236.035291	5281.065599	7.559373	-0.046918	3.940502
236.067342	5289.104788	7.564378	-0.046929	3.943378
236.167555	5297.115919	7.569382	-0.046952	3.946242
236.700368	5305.130950	7.574387	-0.047057	3.949113
236.758215	5313.180496	7.579392	-0.047072	3.951987
236.859170	5321.218944	7.584397	-0.047096	3.954854
237.128193	5329.256011	7.589402	-0.047151	3.957723
237.303192	5337.202687	7.594406	-0.047189	3.960555
237.620467	5345.241345	7.599411	-0.047253	3.963420
237.763722	5353.238069	7.604416	-0.047285	3.966266
237.857211	5361.231546	7.609421	-0.047307	3.969107
237.944528	5369.326983	7.614426	-0.047328	3.971982
238.080456	5377.351199	7.619430	-0.047359	3.974831
238.319739	5385.329675	7.624435	-0.047408	3.977663
238.529261	5393.353252	7.629440	-0.047452	3.980509
238.636484	5401.360092	7.634445	-0.047477	3.983345
239.067199	5409.413272	7.639450	-0.047562	3.986201
239.240649	5417.420712	7.644454	-0.047600	3.989034
239.408999	5425.500475	7.649459	-0.047636	3.991891
239.638031	5433.548810	7.654464	-0.047684	3.994735
239.921993	5441.546460	7.659469	-0.047742	3.997561
240.190726	5449.516916	7.664474	-0.047797	4.000374
240.037258	5457.521109	7.669478	-0.047773	4.003191
240.477446	5465.584835	7.674483	-0.047860	4.006036
240.630978	5473.579458	7.679488	-0.047894	4.008850
240.712917	5481.646954	7.684493	-0.047914	4.011687
241.259888	5489.673696	7.689498	-0.048021	4.014514
241.410355	5497.675868	7.694502	-0.048054	4.017325
241.520215	5505.670368	7.699507	-0.048079	4.020130
241.609810	5513.691001	7.704512	-0.048101	4.022943
241.638781	5521.704785	7.709517	-0.048111	4.025750
241.943056	5529.752342	7.714522	-0.048173	4.028571
242.255764	5537.741011	7.719526	-0.048236	4.031369
243.041765	5545.881152	7.724531	-0.048388	4.034226
243.191951	5553.866037	7.729536	-0.048421	4.037017
243.418819	5561.776272	7.734541	-0.048468	4.039781
243.988631	5569.811747	7.739546	-0.048579	4.042591
244.269457	5577.755086	7.744550	-0.048636	4.045364
244.251120	5585.871769	7.749555	-0.048638	4.048190
244.370018	5593.888745	7.754560	-0.048665	4.050982
244.684953	5601.892333	7.759565	-0.048729	4.053770
244.941179	5609.910304	7.764570	-0.048781	4.056560
244.977673	5617.885458	7.769574	-0.048793	4.059330
245.009588	5625.956260	7.774579	-0.048804	4.062131
245.254635	5633.889729	7.779584	-0.048855	4.064886
245.494534	5641.954157	7.784589	-0.048904	4.067684
245.679880	5649.998508	7.789594	-0.048944	4.070473
245.691193	5658.034746	7.794598	-0.048951	4.073254
245.915475	5666.055272	7.799603	-0.048998	4.076031
246.209482	5674.042429	7.804608	-0.049057	4.078796
246.575373	5682.038598	7.809613	-0.049131	4.081563
246.806047	5690.066528	7.814618	-0.049179	4.084337
246.769020	5698.118737	7.819622	-0.049177	4.087113
247.426219	5706.104742	7.824627	-0.049304	4.089875
247.476116	5714.142831	7.829632	-0.049318	4.092644
247.538203	5722.126033	7.834637	-0.049335	4.095393
247.664078	5730.185707	7.839642	-0.049363	4.098166
247.921325	5738.174065	7.844646	-0.049416	4.100916
248.224517	5746.194322	7.849651	-0.049478	4.103675
248.338255	5754.271001	7.854656	-0.049504	4.106449
248.439448	5762.279016	7.859661	-0.049528	4.109197
248.448601	5770.325977	7.864666	-0.049534	4.111955
248.593125	5778.356863	7.869670	-0.049566	4.114708
248.824442	5786.380831	7.874675	-0.049614	4.117458
249.105041	5794.329014	7.879680	-0.049672	4.120181
249.235618	5802.340189	7.884685	-0.049701	4.122921
249.485399	5810.373398	7.889690	-0.049753	4.125669
249.444149	5818.352280	7.894694	-0.049750	4.128393
249.817021	5826.449507	7.899699	-0.049824	4.131160
249.971965	5834.489679	7.904704	-0.049858	4.133903
250.155139	5842.481088	7.909709	-0.049897	4.136629
250.397043	5850.496842	7.914714	-0.049947	4.139361
250.492621	5858.522288	7.919718	-0.049970	4.142093
250.938163	5866.508552	7.924723	-0.050058	4.144814
251.248724	5874.556469	7.929728	-0.050121	4.147553
251.341320	5882.573327	7.934733	-0.050143	4.150276
251.606237	5890.645633	7.939738	-0.050198	4.153019
251.710319	5898.636874	7.944742	-0.050222	4.155731
251.893781	5906.620516	7.949747	-0.050261	4.158439
251.720433	5914.668678	7.954752	-0.050234	4.161163
252.040531	5922.641597	7.959757	-0.050298	4.163865
252.371158	5930.697956	7.964762	-0.050365	4.166594
252.502742	5938.683286	7.969766	-0.050394	4.169295
252.869010	5946.736267	7.974771	-0.050468	4.172019
252.963371	5954.750054	7.979776	-0.050490	4.174726
253.028902	5962.767263	7.984781	-0.050507	4.177431
253.304408	5970.748533	7.989786	-0.050564	4.180125
253.276674	5978.743121	7.994790	-0.050564	4.182819
253.516030	5986.798182	7.999795	-0.050613	4.185534
253.738205	5994.844284	8.004800	-0.050660	4.188243
253.908398	6002.809137	8.009805	-0.050696	4.190924
254.074717	6010.982805	8.014810	-0.050732	4.193672
254.020391	6018.932704	8.019814	-0.050727	4.196342
254.443680	6026.899595	8.024819	-0.050811	4.199020
254.522689	6034.913252	8.029824	-0.050831	4.201709
254.759094	6042.861036	8.034829	-0.050880	4.204375
255.128950	6050.936637	8.039834	-0.050953	4.207084
255.313668	6058.846035	8.044838	-0.050993	4.209734
255.527480	6066.976183	8.049843	-0.051038	4.212456
255.552539	6075.007182	8.054848	-0.051047	4.215141
255.732926	6082.993774	8.059853	-0.051086	4.217811
256.252396	6090.973488	8.064858	-0.051188	4.220481
256.260472	6099.006437	8.069862	-0.051194	4.223161
256.279908	6107.042292	8.074867	-0.051203	4.225841
256.491405	6115.047638	8.079872	-0.051247	4.228511
256.724763	6123.057501	8.084877	-0.051296	4.231181
256.869830	6131.135132	8.089882	-0.051328	4.233871
256.969311	6139.146044	8.094886	-0.051351	4.236537
257.335932	6147.105564	8.099891	-0.051424	4.239186
257.539868	6155.175424	8.104896	-0.051467	4.241869
257.386084	6163.120401	8.109901	-0.051444	4.244505
257.652323	6171.196874	8.114906	-0.051498	4.247187
257.727676	6179.184977	8.119910	-0.051517	4.249837
257.805138	6187.236476	8.124915	-0.051537	4.252505
258.098085	6195.279623	8.129920	-0.051596	4.255171
258.178714	6203.272379	8.134925	-0.051616	4.257817
258.520703	6211.308411	8.139930	-0.051685	4.260478
258.727402	6219.262536	8.144934	-0.051729	4.263109
259.014650	6227.347155	8.149939	-0.051787	4.265782
259.088153	6235.369772	8.154944	-0.051806	4.268431
259.161325	6243.359553	8.159949	-0.051824	4.271068
259.640740	6251.473501	8.164954	-0.051919	4.273747
259.647127	6259.487436	8.169958	-0.051925	4.276388
259.659514	6267.486263	8.174963	-0.051932	4.279022
259.921872	6275.458997	8.179968	-0.051986	4.281648
260.076256	6283.434716	8.184973	-0.052020	4.284272
260.169436	6291.501493	8.189978	-0.052042	4.286924
260.102314	6299.454650	8.194982	-0.052035	4.289536
260.351855	6307.511370	8.199987	-0.052086	4.292183
260.667326	6315.556327	8.204992	-0.052150	4.294825
260.825952	6323.562555	8.209997	-0.052184	4.297451
261.165615	6331.544611	8.215002	-0.052253	4.300069
261.099366	6339.585243	8.220006	-0.052245	4.302701
261.209761	6347.591285	8.225011	-0.052271	4.305322
261.462749	6355.651424	8.230016	-0.052323	4.307960
261.763843	6363.619947	8.235021	-0.052384	4.310567
261.897042	6371.660400	8.240026	-0.052414	4.313195
262.045613	6379.702594	8.245030	-0.052447	4.315821
262.316322	6387.677104	8.250035	-0.052502	4.318425
262.511837	6395.705168	8.255040	-0.052543	4.321044
262.546966	6403.703436	8.260045	-0.052555	4.323651
262.922073	6411.753685	8.265050	-0.052630	4.326275
263.048482	6419.757825	8.270054	-0.052658	4.328881
263.083650	6427.789953	8.275059	-0.052670	4.331494
263.172696	6435.810419	8.280064	-0.052691	4.334102
263.502329	6443.828698	8.285069	-0.052758	4.336709
263.766125	6451.802356	8.290074	-0.052812	4.339299
263.645954	6459.829366	8.295078	-0.052795	4.341903
263.750183	6467.816044	8.300083	-0.052819	4.344494
263.937512	6475.892552	8.305088	-0.052859	4.347112
264.286824	6483.842474	8.310093	-0.052929	4.349690
264.528777	6491.971155	8.315098	-0.052979	4.352322
264.521773	6500.076053	8.320102	-0.052983	4.354944
264.734296	6508.027908	8.325107	-0.053027	4.357517
264.905357	6515.924475	8.330112	-0.053064	4.360069
265.011212	6523.955633	8.335117	-0.053089	4.362663
265.204259	6531.962850	8.340122	-0.053130	4.365249
265.319737	6539.984120	8.345126	-0.053156	4.367836
265.638363	6547.973436	8.350131	-0.053221	4.370414
265.779004	6556.035869	8.355136	-0.053252	4.373012
265.580955	6564.037626	8.360141	-0.053220	4.375587
266.001077	6572.078362	8.365146	-0.053303	4.378176
266.194410	6580.064034	8.370150	-0.053344	4.380746
266.358883	6588.128843	8.375155	-0.053380	4.383338
266.448200	6596.109403	8.380160	-0.053401	4.385902
266.722547	6604.092418	8.385165	-0.053457	4.388466
266.991519	6612.173761	8.390170	-0.053513	4.391060
266.799383	6620.223066	8.395174	-0.053482	4.393640
267.070277	6628.241928	8.400179	-0.053537	4.396211
267.132716	6636.214468	8.405184	-0.053554	4.398764
267.393559	6644.193279	8.410189	-0.053607	4.401320
267.580041	6652.197575	8.415194	-0.053647	4.403881
267.754890	6660.232199	8.420198	-0.053685	4.406450
267.696894	6668.249879	8.425203	-0.053679	4.409012
267.777893	6676.309143	8.430208	-0.053699	4.411585
268.104488	6684.304754	8.435213	-0.053765	4.414138
268.297857	6692.384528	8.440218	-0.053806	4.416716
268.256934	6700.359979	8.445222	-0.053803	4.419258
268.555708	6708.384937	8.450227	-0.053864	4.421816
268.740283	6716.402618	8.455232	-0.053903	4.424370
268.912477	6724.394766	8.460237	-0.053940	4.426913
269.079396	6732.441746	8.465242	-0.053976	4.429473
269.206383	6740.460611	8.470246	-0.054005	4.432022
269.383785	6748.521791	8.475251	-0.054043	4.434584
269.619036	6756.559368	8.480256	-0.054092	4.437136
269.800835	6764.464594	8.485261	-0.054131	4.439645
269.989256	6772.521029	8.490266	-0.054171	4.442200
269.986366	6780.491089	8.495270	-0.054175	4.444726
270.198291	6788.524031	8.500275	-0.054220	4.447271
270.461817	6796.552128	8.505280	-0.054274	4.449813
270.633149	6804.595959	8.510285	-0.054311	4.452359
270.902757	6812.630411	8.515290	-0.054366	4.454900
270.916825	6820.628209	8.520294	-0.054374	4.457427
271.159041	6828.621886	8.525299	-0.054424	4.459953
271.208180	6836.629404	8.530304	-0.054438	4.462480
271.398581	6844.636877	8.535309	-0.054478	4.465007
271.687343	6852.685486	8.540314	-0.054537	4.467545
271.550738	6860.662299	8.545318	-0.054517	4.470058
271.818198	6868.734296	8.550323	-0.054571	4.472601
272.117738	6876.779892	8.555328	-0.054632	4.475134
272.148971	6884.738712	8.560333	-0.054643	4.477638
272.418732	6892.752161	8.565338	-0.054698	4.480158
272.566026	6900.762547	8.570343	-0.054731	4.482675
272.718012	6908.719772	8.575347	-0.054764	4.485174
272.929837	6916.826192	8.580352	-0.054808	4.487719
273.009197	6924.792226	8.585357	-0.054828	4.490218
273.313165	6932.875171	8.590362	-0.054890	4.492753
273.276570	6940.856325	8.595367	-0.054888	4.495253
273.394080	6948.903346	8.600371	-0.054915	4.497773
273.723943	6956.863236	8.605376	-0.054981	4.500265
273.825974	6964.871591	8.610381	-0.055005	4.502770
273.930437	6972.903413	8.615386	-0.055030	4.505281
274.242568	6980.952034	8.620391	-0.055093	4.507797
274.427335	6988.907301	8.625395	-0.055132	4.510281
274.578627	6997.040418	8.630400	-0.055165	4.512820
274.589826	7005.027074	8.635405	-0.055172	4.515311
274.994963	7013.045240	8.640410	-0.055253	4.517811
274.901064	7020.976450	8.645415	-0.055240	4.520282
275.131389	7029.006937	8.650419	-0.055288	4.522783
275.350834	7037.001903	8.655424	-0.055334	4.525271
275.459000	7045.031232	8.660429	-0.055359	4.527769
275.585747	7053.043826	8.665434	-0.055388	4.530260
275.749084	7061.103876	8.670439	-0.055423	4.532765
276.203670	7069.133471	8.675443	-0.055513	4.535259
276.273702	7077.129718	8.680448	-0.055531	4.537740
276.219602	7085.089813	8.685453	-0.055526	4.540209
276.561994	7093.182974	8.690458	-0.055595	4.542719
276.471657	7101.121812	8.695463	-0.055583	4.545178
276.756362	7109.192061	8.700467	-0.055641	4.547678
277.011609	7117.190329	8.705472	-0.055693	4.550154
277.217928	7125.193295	8.710477	-0.055737	4.552629
277.271977	7133.265047	8.715482	-0.055752	4.555125
277.521701	7141.291876	8.720487	-0.055803	4.557605
277.768981	7149.231168	8.725491	-0.055854	4.560057
277.829360	7157.290936	8.730496	-0.055871	4.562545
277.861073	7165.224647	8.735501	-0.055882	4.564992
278.219477	7173.301231	8.740506	-0.055953	4.567482
278.232465	7181.278157	8.745511	-0.055961	4.569940
278.247948	7189.335433	8.750515	-0.055969	4.572422
278.586870	7197.386983	8.755520	-0.056037	4.574900
278.904744	7205.411631	8.760525	-0.056101	4.577369
278.925840	7213.422232	8.765530	-0.056110	4.579832
279.163104	7221.416304	8.770535	-0.056159	4.582289
279.542561	7229.413427	8.775539	-0.056235	4.584745
279.509005	7237.469769	8.780544	-0.056234	4.587218
279.414673	7245.434885	8.785549	-0.056221	4.589662
279.953880	7253.531474	8.790554	-0.056326	4.592145
280.068356	7261.539547	8.795559	-0.056353	4.594599
280.395615	7269.570031	8.800563	-0.056419	4.597059
280.771942	7277.533490	8.805568	-0.056494	4.599497
280.896979	7285.562793	8.810573	-0.056522	4.601953
281.104037	7293.504477	8.815578	-0.056565	4.604382
281.152544	7301.557805	8.820583	-0.056580	4.606843
281.238786	7309.585809	8.825587	-0.056601	4.609296
281.320009	7317.610969	8.830592	-0.056621	4.611746
281.524359	7325.637375	8.835597	-0.056664	4.614195
281.795064	7333.680438	8.840602	-0.056719	4.616648
281.809001	7341.640691	8.845607	-0.056727	4.619075
281.970815	7349.649315	8.850611	-0.056762	4.621514
282.189022	7357.661264	8.855616	-0.056808	4.623954
282.343163	7365.676443	8.860621	-0.056841	4.626393
282.584277	7373.730934	8.865626	-0.056891	4.628843
282.611034	7381.748397	8.870631	-0.056901	4.631280
283.049453	7389.740968	8.875635	-0.056988	4.633709
283.231971	7397.829990	8.880640	-0.057027	4.636165
283.032204	7405.806345	8.885645	-0.056995	4.638586
283.275306	7413.764103	8.890650	-0.057045	4.641000
283.360089	7421.775161	8.895655	-0.057066	4.643429
283.399825	7429.759421	8.900659	-0.057078	4.645849
283.579001	7437.815274	8.905664	-0.057116	4.648288
283.927766	7445.808892	8.910669	-0.057186	4.650708
284.265558	7453.891414	8.915674	-0.057254	4.653153
284.274758	7461.917319	8.920679	-0.057261	4.655580
284.507420	7469.908962	8.925683	-0.057309	4.657995
284.728586	7477.921346	8.930688	-0.057355	4.660415
284.727205	7485.909178	8.935693	-0.057360	4.662827
284.929696	7493.927873	8.940698	-0.057403	4.665247
285.052175	7501.947361	8.945703	-0.057431	4.667665
285.371856	7509.964710	8.950707	-0.057495	4.670082
285.190049	7518.049258	8.955712	-0.057466	4.672518
285.520881	7526.061685	8.960717	-0.057533	4.674930
285.649936	7534.133376	8.965722	-0.057562	4.677360
285.525516	7542.027343	8.970727	-0.057544	4.679734
286.074575	7550.041171	8.975731	-0.057651	4.682143
286.158836	7558.006806	8.980736	-0.057672	4.684537
285.969951	7566.054995	8.985741	-0.057642	4.686954
286.488986	7574.054388	8.990746	-0.057743	4.689355
286.723414	7582.124983	8.995751	-0.057792	4.691776
287.027539	7590.148234	9.000755	-0.057854	4.694181
287.104931	7598.189834	9.005760	-0.057873	4.696592
287.333433	7606.157422	9.010765	-0.057920	4.698978
287.656109	7614.187184	9.015770	-0.057986	4.701382
287.478071	7622.145541	9.020775	-0.057957	4.703764
287.706968	7630.172509	9.025779	-0.058005	4.706164
287.965011	7638.255079	9.030784	-0.058058	4.708580
288.007396	7646.193897	9.035789	-0.058071	4.710952
288.162238	7654.255802	9.040794	-0.058105	4.713360
288.475648	7662.283451	9.045799	-0.058168	4.715755
288.474250	7670.276015	9.050803	-0.058173	4.718140
288.675279	7678.293230	9.055808	-0.058215	4.720530
288.832115	7686.286961	9.060813	-0.058250	4.722912
289.365707	7694.303924	9.065818	-0.058354	4.725299
289.176353	7702.321625	9.070823	-0.058324	4.727687
289.356299	7710.352043	9.075827	-0.058362	4.730076
289.600410	7718.388264	9.080832	-0.058413	4.732465
289.619675	7726.405433	9.085837	-0.058421	4.734849
289.755039	7734.463552	9.090842	-0.058451	4.737243
289.917405	7742.396747	9.095847	-0.058487	4.739598
290.004002	7750.465725	9.100851	-0.058508	4.741993
290.255827	7758.409004	9.105856	-0.058560	4.744349
290.420526	7766.461757	9.110861	-0.058595	4.746736
290.770708	7774.492225	9.115866	-0.058666	4.749115
290.774947	7782.506127	9.120871	-0.058671	4.751489
291.076127	7790.554846	9.125875	-0.058732	4.753871
291.177242	7798.600134	9.130880	-0.058756	4.756252
291.228852	7806.567622	9.135885	-0.058771	4.758608
291.382922	7814.550876	9.140890	-0.058805	4.760968
291.597348	7822.565310	9.145895	-0.058849	4.763335
291.765679	7830.575850	9.150899	-0.058886	4.765701
291.876622	7838.627805	9.155904	-0.058912	4.768077
292.261442	7846.612170	9.160909	-0.058988	4.770431
292.633936	7854.712724	9.165914	-0.059063	4.772819
292.537555	7862.634393	9.170919	-0.059050	4.775154
292.620324	7870.689497	9.175923	-0.059070	4.777527
292.902989	7878.653779	9.180928	-0.059128	4.779871
292.906669	7886.692533	9.185933	-0.059133	4.782237
293.085479	7894.665526	9.190938	-0.059172	4.784581
293.115891	7902.754057	9.195943	-0.059182	4.786959
293.520978	7910.704281	9.200947	-0.059263	4.789294
293.656056	7918.799223	9.205952	-0.059293	4.791671
293.638737	7926.774743	9.210957	-0.059295	4.794013
293.918400	7934.840530	9.215962	-0.059352	4.796378
294.088316	7942.765015	9.220967	-0.059388	4.798701
294.420880	7950.806687	9.225971	-0.059455	4.801057
294.566833	7958.818647	9.230976	-0.059487	4.803404
294.791859	7966.805971	9.235981	-0.059534	4.805742
294.878601	7974.848427	9.240986	-0.059555	4.808096
294.972810	7982.838412	9.245991	-0.059578	4.810433
295.112055	7990.416579	9.250995	-0.059609	4.812648
295.183622	7995.174771	9.256000	-0.059625	4.814039
295.148370	7997.592743	9.261005	-0.059620	4.814746
295.551637	7999.041694	9.266010	-0.059695	4.815167
295.566084	7999.580422	9.271015	-0.059698	4.815325
295.604291	7999.827855	9.276019	-0.059705	4.815397
295.785401	8000.167404	9.281024	-0.059739	4.815495
295.965385	8000.275067	9.286029	-0.059772	4.815526
296.017075	8000.106002	9.291034	-0.059782	4.815476
296.039443	8000.133064	9.296039	-0.059786	4.815484
296.012708	8000.237321	9.301043	-0.059781	4.815514
296.206811	8000.060986	9.306048	-0.059816	4.815462
296.240437	8000.434444	9.311053	-0.059823	4.815571
296.337507	8000.166749	9.316058	-0.059840	4.815492
296.397052	8000.185876	9.321063	-0.059851	4.815498
296.536603	8000.183883	9.326067	-0.059877	4.815496
296.620908	8000.217310	9.331072	-0.059892	4.815506
296.623708	8000.423569	9.336077	-0.059893	4.815566
296.759915	8000.036840	9.341082	-0.059918	4.815452
296.644545	8000.292440	9.346087	-0.059896	4.815528
296.894777	8000.187553	9.351091	-0.059943	4.815496
296.921341	8000.288417	9.356096	-0.059947	4.815525
296.875275	8000.196809	9.361101	-0.059938	4.815498
297.030394	8000.170496	9.366106	-0.059967	4.815490
297.179503	8000.147290	9.371111	-0.059995	4.815483
297.027715	8000.388401	9.376115	-0.059966	4.815554
297.180315	8000.146195	9.381120	-0.059994	4.815482
297.351507	8000.100913	9.386125	-0.060026	4.815468
297.318656	8000.125997	9.391130	-0.060020	4.815476
297.194854	8000.006394	9.396135	-0.059996	4.815441
297.258156	7999.947579	9.401139	-0.060008	4.815424
297.252924	7999.911142	9.406144	-0.060007	4.815413
297.094224	8000.083750	9.411149	-0.059977	4.815464
297.319565	7999.934641	9.416154	-0.060019	4.815420
297.409006	8000.102792	9.421159	-0.060035	4.815468
297.403309	8000.056730	9.426163	-0.060034	4.815455
297.589909	8000.025593	9.431168	-0.060068	4.815445
297.440330	8000.144924	9.436173	-0.060040	4.815481
297.449985	8000.106595	9.441178	-0.060042	4.815469
297.506039	8000.187643	9.446183	-0.060052	4.815493
297.600504	8000.140027	9.451187	-0.060069	4.815478
297.558810	8000.071999	9.456192	-0.060061	4.815459
297.326527	8000.227366	9.461197	-0.060018	4.815505
297.540409	8000.111194	9.466202	-0.060058	4.815470
297.524362	8000.163270	9.471207	-0.060054	4.815486
297.479708	8000.282194	9.476211	-0.060046	4.815521
297.743797	8000.027934	9.481216	-0.060095	4.815445
297.646982	8000.206908	9.486221	-0.060077	4.815498
297.659110	8000.120533	9.491226	-0.060079	4.815473
297.507974	8000.228084	9.496231	-0.060050	4.815505
297.720284	8000.134326	9.501235	-0.060090	4.815476
297.818410	8000.111347	9.506240	-0.060108	4.815469
297.680180	8000.146448	9.511245	-0.060082	4.815480
297.869403	7999.972165	9.516250	-0.060117	4.815428
297.976619	7999.979256	9.521255	-0.060136	4.815430
297.884486	8000.227765	9.526259	-0.060119	4.815503
297.991189	7999.947400	9.531264	-0.060139	4.815420
297.804058	8000.166559	9.536269	-0.060104	4.815485
297.931636	7999.962408	9.541274	-0.060127	4.815425
297.837170	7999.978996	9.546279	-0.060109	4.815430
297.975759	8000.109491	9.551283	-0.060135	4.815468
297.906532	8000.108330	9.556288	-0.060122	4.815468
297.771293	8000.097531	9.561293	-0.060096	4.815465
297.829716	8000.138012	9.566298	-0.060107	4.815477
297.941408	8000.221047	9.571303	-0.060128	4.815501
297.944353	8000.131315	9.576307	-0.060128	4.815474
298.099086	7999.998138	9.581312	-0.060156	4.815435
298.038991	8000.134974	9.586317	-0.060145	4.815475
298.174027	7999.940563	9.591322	-0.060170	4.815418
298.271873	8000.109924	9.596327	-0.060188	4.815467
298.311501	8000.078501	9.601331	-0.060195	4.815457
298.220976	7999.889986	9.606336	-0.060178	4.815403
297.943690	8000.043543	9.611341	-0.060126	4.815449
298.191527	7999.829621	9.616346	-0.060172	4.815385
298.171363	7999.912618	9.621351	-0.060168	4.815409
298.095763	7999.965849	9.626355	-0.060154	4.815425
298.220823	7999.949726	9.631360	-0.060177	4.815420
297.999778	8000.105279	9.636365	-0.060136	4.815467
298.220254	7999.916551	9.641370	-0.060176	4.815410
298.167003	7999.961602	9.646375	-0.060166	4.815424
298.313567	8000.021703	9.651379	-0.060193	4.815441
298.207283	7999.964365	9.656384	-0.060173	4.815424
298.160971	8000.137760	9.661389	-0.060165	4.815475
298.298032	8000.031005	9.666394	-0.060190	4.815444
298.166801	7999.997833	9.671399	-0.060165	4.815434
298.281439	8000.242274	9.676403	-0.060186	4.815505
298.260754	8000.002549	9.681408	-0.060182	4.815435
298.300585	8000.077987	9.686413	-0.060189	4.815457
298.403669	7999.828551	9.691418	-0.060208	4.815384
298.301943	7999.973249	9.696423	-0.060189	4.815427
298.159571	7999.979430	9.701427	-0.060162	4.815429
298.658234	7999.809181	9.706432	-0.060255	4.815377
298.589049	8000.087990	9.711437	-0.060242	4.815459
298.385589	7999.852732	9.716442	-0.060204	4.815391
298.139871	8000.216252	9.721447	-0.060158	4.815498
298.269901	8000.217309	9.726451	-0.060182	4.815498
298.297385	8000.002956	9.731456	-0.060187	4.815435
298.234943	8000.046787	9.736461	-0.060175	4.815449
298.398755	7999.902005	9.741466	-0.060205	4.815405
298.271933	7999.949049	9.746471	-0.060181	4.815420
298.356818	7999.988898	9.751475	-0.060197	4.815431
298.580936	7999.979752	9.756480	-0.060238	4.815427
298.416218	8000.157607	9.761485	-0.060208	4.815480
298.450554	7999.991454	9.766490	-0.060214	4.815431
298.847867	8000.199953	9.771495	-0.060288	4.815490
298.589412	8000.130485	9.776499	-0.060239	4.815471
298.433638	7999.938755	9.781504	-0.060210	4.815416
298.480317	8000.011101	9.786509	-0.060218	4.815437
298.736960	7999.841134	9.791514	-0.060266	4.815386
298.665585	7999.922219	9.796519	-0.060252	4.815410
298.513954	8000.140896	9.801523	-0.060224	4.815475
298.616799	7999.944884	9.806528	-0.060243	4.815417
298.497203	8000.023035	9.811533	-0.060220	4.815440
298.577309	7999.908930	9.816538	-0.060235	4.815407
298.476717	8000.006629	9.821543	-0.060216	4.815436
298.580068	8000.085253	9.826547	-0.060235	4.815458
298.557800	7999.975870	9.831552	-0.060231	4.815426
298.727144	8000.211598	9.836557	-0.060262	4.815494
298.814814	8000.047391	9.841562	-0.060278	4.815446
298.799687	8000.053534	9.846567	-0.060275	4.815448
298.586823	8000.027562	9.851571	-0.060235	4.815441
298.947545	7999.949074	9.856576	-0.060302	4.815417
298.708881	8000.153494	9.861581	-0.060258	4.815478
298.682314	7999.977786	9.866586	-0.060252	4.815426
298.662498	8000.140935	9.871591	-0.060249	4.815474
298.678755	8000.080273	9.876595	-0.060251	4.815456
298.688964	8000.130646	9.881600	-0.060253	4.815471
298.517952	8000.228253	9.886605	-0.060221	4.815500
298.920765	7999.973073	9.891610	-0.060296	4.815424
299.008681	7999.977709	9.896615	-0.060312	4.815425
298.886455	8000.051544	9.901619	-0.060289	4.815447
299.081542	7999.960706	9.906624	-0.060325	4.815419
299.213671	7999.968209	9.911629	-0.060349	4.815421
298.942815	7999.924183	9.916634	-0.060299	4.815409
298.930989	8000.117384	9.921639	-0.060296	4.815466
299.110875	7999.976071	9.926643	-0.060330	4.815424
298.863318	7999.764662	9.931648	-0.060283	4.815363
298.705157	7999.977888	9.936653	-0.060254	4.815426
298.903550	7999.953358	9.941658	-0.060290	4.815418
298.930054	8000.011479	9.946663	-0.060295	4.815435
298.751912	8000.057676	9.951667	-0.060262	4.815449
298.955831	7999.943475	9.956672	-0.060299	4.815415
298.941947	8000.013754	9.961677	-0.060297	4.815436
298.831172	7999.981986	9.966682	-0.060276	4.815427
298.903666	7999.969271	9.971687	-0.060289	4.815423
298.974876	7999.949054	9.976691	-0.060302	4.815417
299.021735	7999.932710	9.981696	-0.060310	4.815412
298.958118	8000.065215	9.986701	-0.060299	4.815451
299.130508	7999.984689	9.991706	-0.060330	4.815426
299.220049	7999.951951	9.996711	-0.060347	4.815416
299.117795	7999.992989	10.001715	-0.060328	4.815429
299.128143	7999.921544	10.006720	-0.060329	4.815408
299.092706	8000.079092	10.011725	-0.060322	4.815454
299.173549	7999.844246	10.016730	-0.060337	4.815385
299.088159	7999.984941	10.021735	-0.060321	4.815427
299.195483	7999.961045	10.026739	-0.060341	4.815419
299.338675	7999.951633	10.031744	-0.060367	4.815416
299.167831	8000.135801	10.036749	-0.060335	4.815470
299.114068	7999.975672	10.041754	-0.060325	4.815424
299.137764	7999.989936	10.046759	-0.060329	4.815428
299.098155	7999.962547	10.051763	-0.060322	4.815420
299.371373	7999.937114	10.056768	-0.060372	4.815411
299.225490	7999.920796	10.061773	-0.060345	4.815407
299.134815	7999.962025	10.066778	-0.060328	4.815420
299.271915	7999.949306	10.071783	-0.060353	4.815415
299.153965	8000.006114	10.076787	-0.060331	4.815433
299.302370	7999.936946	10.081792	-0.060358	4.815412
299.204364	8000.021867	10.086797	-0.060340	4.815437
299.358132	7999.835242	10.091802	-0.060368	4.815382
299.333964	7999.932066	10.096807	-0.060364	4.815410
299.168800	8000.005192	10.101811	-0.060333	4.815432
299.220782	7999.835054	10.106816	-0.060342	4.815382
299.213312	7999.958869	10.111821	-0.060340	4.815419
299.311558	7999.871776	10.116826	-0.060358	4.815393
299.389916	7999.964949	10.121831	-0.060373	4.815419
299.354210	8000.027388	10.126835	-0.060366	4.815438
299.374876	7999.882379	10.131840	-0.060370	4.815395
299.304784	7999.956005	10.136845	-0.060356	4.815417
299.235243	7999.909957	10.141850	-0.060343	4.815404
299.425117	7999.893835	10.146855	-0.060378	4.815399
299.192763	8000.047067	10.151859	-0.060335	4.815444
299.427554	7999.952609	10.156864	-0.060378	4.815416
299.434735	7999.812721	10.161869	-0.060379	4.815375
299.449421	7999.939039	10.166874	-0.060382	4.815412
299.206149	7999.865547	10.171879	-0.060336	4.815391
299.193874	7999.940127	10.176883	-0.060334	4.815413
299.643067	7999.839588	10.181888	-0.060417	4.815382
299.220086	7999.920216	10.186893	-0.060338	4.815407
299.249337	7999.882210	10.191898	-0.060344	4.815396
299.446225	7999.943142	10.196903	-0.060380	4.815413
299.343552	7999.886930	10.201907	-0.060361	4.815397
299.181214	7999.871410	10.206912	-0.060330	4.815393
299.312666	7999.990036	10.211917	-0.060355	4.815427
299.411948	8000.018369	10.216922	-0.060373	4.815435
299.253660	8000.006121	10.221927	-0.060343	4.815432
299.481310	7999.833538	10.226931	-0.060385	4.815381
299.623944	7999.945937	10.231936	-0.060412	4.815413
299.321573	7999.983673	10.236941	-0.060355	4.815425
299.419953	7999.940395	10.241946	-0.060373	4.815412
299.457358	7999.810623	10.246951	-0.060380	4.815374
299.522832	8000.082041	10.251955	-0.060392	4.815453
299.501291	7999.974805	10.256960	-0.060388	4.815422
299.398266	7999.974154	10.261965	-0.060368	4.815422
299.451827	8000.041272	10.266970	-0.060378	4.815442
299.406975	7999.947543	10.271975	-0.060369	4.815414
299.312052	7999.989771	10.276979	-0.060352	4.815427
299.570016	7999.906381	10.281984	-0.060399	4.815402
299.575304	8000.022927	10.286989	-0.060400	4.815436
299.504000	7999.911664	10.291994	-0.060387	4.815404
299.617312	7999.883593	10.296999	-0.060407	4.815395
299.412424	8000.026592	10.302003	-0.060369	4.815438
299.516941	7999.958838	10.307008	-0.060388	4.815417
299.580080	7999.999398	10.312013	-0.060400	4.815429
299.610217	8000.059718	10.317018	-0.060405	4.815446
299.734378	7999.828790	10.322023	-0.060428	4.815378
299.500916	7999.939260	10.327027	-0.060384	4.815412
299.680896	7999.846035	10.332032	-0.060418	4.815384
299.415253	7999.951699	10.337037	-0.060368	4.815416
299.616639	7999.984923	10.342042	-0.060405	4.815424
299.757526	7999.953033	10.347047	-0.060431	4.815414
299.585873	7999.979033	10.352051	-0.060399	4.815423
299.605711	7999.838285	10.357056	-0.060403	4.815382
299.747301	7999.994481	10.362061	-0.060429	4.815427
299.688317	7999.956087	10.367066	-0.060418	4.815416
299.662162	7999.932126	10.372071	-0.060412	4.815409
299.524307	7999.972576	10.377075	-0.060387	4.815421
299.816592	7999.828843	10.382080	-0.060441	4.815378
299.849544	7999.923404	10.387085	-0.060447	4.815405
299.794298	7999.849808	10.392090	-0.060436	4.815384
299.882642	7999.971999	10.397095	-0.060452	4.815419
299.869667	7999.849943	10.402099	-0.060450	4.815384
299.707812	7999.913507	10.407104	-0.060419	4.815403
299.496748	8000.046787	10.412109	-0.060380	4.815443
299.737908	8000.011208	10.417114	-0.060425	4.815432
299.811270	7999.847833	10.422119	-0.060438	4.815384
299.649224	7999.965892	10.427123	-0.060408	4.815419
299.836277	7999.940106	10.432128	-0.060442	4.815410
300.009771	8000.045537	10.437133	-0.060474	4.815440
299.904909	7999.828995	10.442138	-0.060454	4.815378
299.794126	7999.941489	10.447143	-0.060434	4.815411
299.933333	8000.142530	10.452147	-0.060460	4.815469
299.861295	7999.814325	10.457152	-0.060446	4.815374
299.736306	7999.951162	10.462157	-0.060422	4.815414
299.880905	7999.854148	10.467162	-0.060449	4.815385
299.818445	7999.963164	10.472167	-0.060437	4.815417
299.669452	8000.079303	10.477171	-0.060409	4.815452
299.990733	7999.839872	10.482176	-0.060469	4.815380
300.014461	8000.040075	10.487181	-0.060473	4.815439
300.112579	8000.056635	10.492186	-0.060491	4.815443
299.965689	7999.878938	10.497191	-0.060463	4.815392
300.001280	8000.005603	10.502195	-0.060470	4.815429
299.981176	7999.921899	10.507200	-0.060466	4.815404
299.613062	7999.970305	10.512205	-0.060397	4.815420
300.019606	7999.936386	10.517210	-0.060473	4.815409
300.013648	7999.935199	10.522215	-0.060471	4.815408
299.992739	7999.834385	10.527219	-0.060467	4.815379
299.909089	7999.852220	10.532224	-0.060451	4.815385
299.878873	7999.925436	10.537229	-0.060445	4.815406
299.994495	7999.836492	10.542234	-0.060467	4.815380
300.169392	7999.855388	10.547239	-0.060499	4.815384
300.108395	7999.928096	10.552243	-0.060488	4.815406
300.021612	7999.845430	10.557248	-0.060471	4.815382
299.940133	7999.931692	10.562253	-0.060456	4.815408
299.949249	7999.740542	10.567258	-0.060457	4.815352
300.005359	7999.872887	10.572263	-0.060467	4.815390
299.836128	7999.933123	10.577267	-0.060436	4.815409
300.099323	7999.874398	10.582272	-0.060485	4.815390
300.046687	7999.961136	10.587277	-0.060475	4.815416
300.086816	7999.921171	10.592282	-0.060482	4.815404
300.057547	7999.851209	10.597287	-0.060476	4.815384
299.931735	8000.088483	10.602291	-0.060453	4.815454
300.184759	7999.852200	10.607296	-0.060499	4.815383
300.058745	7999.990090	10.612301	-0.060476	4.815424
300.024828	8000.117745	10.617306	-0.060469	4.815462
300.213291	7999.913523	10.622311	-0.060504	4.815401
300.047420	7999.949236	10.627315	-0.060473	4.815412
300.028835	7999.805716	10.632320	-0.060469	4.815370
300.041784	7999.926663	10.637325	-0.060471	4.815406
299.915036	7999.974777	10.642330	-0.060448	4.815420
300.020183	7999.936953	10.647335	-0.060467	4.815409
300.064703	7999.945149	10.652339	-0.060475	4.815411
300.299669	7999.890232	10.657344	-0.060518	4.815394
300.109088	8000.009959	10.662349	-0.060483	4.815430
300.325709	7999.867113	10.667354	-0.060523	4.815387
300.118058	7999.871148	10.672359	-0.060484	4.815389
299.961603	8000.060897	10.677363	-0.060455	4.815445
300.070627	7999.873531	10.682368	-0.060475	4.815390
300.010711	7999.981522	10.687373	-0.060463	4.815422
300.095331	8000.059840	10.692378	-0.060479	4.815444
300.138622	7999.820095	10.697383	-0.060487	4.815374
300.245476	7999.960759	10.702387	-0.060506	4.815415
300.197775	7999.812483	10.707392	-0.060497	4.815372
300.102516	7999.928439	10.712397	-0.060479	4.815406
300.120779	7999.930858	10.717402	-0.060483	4.815407
300.400130	7999.882017	10.722407	-0.060534	4.815391
300.274490	7999.868170	10.727411	-0.060511	4.815388
300.305249	7999.908196	10.732416	-0.060516	4.815399
300.385411	7999.822942	10.737421	-0.060531	4.815374
300.257215	7999.843248	10.742426	-0.060507	4.815380
300.295074	7999.943234	10.747431	-0.060514	4.815409
300.295145	7999.941078	10.752435	-0.060513	4.815409
300.359521	7999.814955	10.757440	-0.060525	4.815372
300.167888	7999.980615	10.762445	-0.060489	4.815421
300.127362	7999.863448	10.767450	-0.060482	4.815387
300.265875	7999.820832	10.772455	-0.060507	4.815374
300.037241	7999.921764	10.777459	-0.060464	4.815404
299.980195	7999.838520	10.782464	-0.060453	4.815380
300.180766	7999.977524	10.787469	-0.060491	4.815420
300.214242	7999.952410	10.792474	-0.060497	4.815413
300.104533	7999.825552	10.797479	-0.060476	4.815376
300.231666	7999.965481	10.802483	-0.060499	4.815416
300.369151	7999.835222	10.807488	-0.060525	4.815378
300.199987	7999.876224	10.812493	-0.060493	4.815390
300.150257	7999.746082	10.817498	-0.060483	4.815353
300.408349	7999.865731	10.822503	-0.060531	4.815386
300.201057	7999.834507	10.827507	-0.060493	4.815378
300.165669	7999.746277	10.832512	-0.060486	4.815353
300.116790	7999.942076	10.837517	-0.060477	4.815410
300.219466	7999.824066	10.842522	-0.060495	4.815375
300.190403	7999.874860	10.847527	-0.060490	4.815390
299.964912	7999.856159	10.852531	-0.060448	4.815386
300.248765	7999.830902	10.857536	-0.060500	4.815377
300.154955	8000.094352	10.862541	-0.060483	4.815454
300.197846	7999.968942	10.867546	-0.060490	4.815418
300.281695	7999.811082	10.872551	-0.060506	4.815371
300.062387	8000.069255	10.877555	-0.060465	4.815448
300.263952	7999.849221	10.882560	-0.060502	4.815382
300.461967	7999.947576	10.887565	-0.060539	4.815410
300.228444	7999.933016	10.892570	-0.060495	4.815407
300.310710	7999.815737	10.897575	-0.060510	4.815372
300.401748	8000.043768	10.902579	-0.060527	4.815439
300.595955	7999.762700	10.907584	-0.060563	4.815355
300.353665	7999.925386	10.912589	-0.060517	4.815404
300.305010	7999.855104	10.917594	-0.060508	4.815384
300.575021	7999.832824	10.922599	-0.060558	4.815376
300.569972	7999.841270	10.927603	-0.060557	4.815379
300.329930	7999.743252	10.932608	-0.060512	4.815351
300.373272	7999.938435	10.937613	-0.060520	4.815408
300.460170	7999.837262	10.942618	-0.060536	4.815378
300.419580	7999.783142	10.947623	-0.060528	4.815362
300.311301	8000.011089	10.952627	-0.060508	4.815429
300.456076	7999.841410	10.957632	-0.060534	4.815379
300.278989	7999.818165	10.962637	-0.060501	4.815373
300.247699	7999.958686	10.967642	-0.060495	4.815414
300.307929	7999.812191	10.972647	-0.060506	4.815371
300.335720	7999.944070	10.977651	-0.060511	4.815410
300.415404	7999.845984	10.982656	-0.060526	4.815381
300.282549	7999.999790	10.987661	-0.060501	4.815426
300.403424	8000.011383	10.992666	-0.060523	4.815429
300.545755	7999.911125	10.997671	-0.060549	4.815399
300.466076	7999.939711	11.002675	-0.060534	4.815408
300.633997	7999.811022	11.007680	-0.060565	4.815370
300.516355	7999.877453	11.012685	-0.060543	4.815390
300.146445	8000.072230	11.017690	-0.060474	4.815448
300.378949	7999.882627	11.022695	-0.060517	4.815392
300.332910	7999.888259	11.027699	-0.060508	4.815394
300.359387	7999.811736	11.032704	-0.060513	4.815371
300.432185	7999.944358	11.037709	-0.060526	4.815409
300.358901	7999.837335	11.042714	-0.060512	4.815379
300.384544	7999.916817	11.047719	-0.060517	4.815402
300.376430	7999.835448	11.052723	-0.060515	4.815378
300.609062	7999.848885	11.057728	-0.060558	4.815381
300.357075	7999.832952	11.062733	-0.060511	4.815377
300.449849	7999.886826	11.067738	-0.060528	4.815393
300.578902	7999.875044	11.072743	-0.060552	4.815389
300.337996	7999.844333	11.077747	-0.060507	4.815381
300.540033	7999.848716	11.082752	-0.060544	4.815381
300.479387	7999.806020	11.087757	-0.060533	4.815369
300.511748	7999.942249	11.092762	-0.060539	4.815409
300.624058	7999.848975	11.097767	-0.060559	4.815381
300.521916	7999.828035	11.102771	-0.060540	4.815375
300.661249	7999.738413	11.107776	-0.060566	4.815348
300.758627	7999.988990	11.112781	-0.060584	4.815421
300.538518	7999.854965	11.117786	-0.060543	4.815383
300.702775	7999.822392	11.122791	-0.060573	4.815373
300.703947	7999.805294	11.127795	-0.060573	4.815368
300.687218	7999.834919	11.132800	-0.060570	4.815376
300.597670	7999.831285	11.137805	-0.060553	4.815376
300.532694	7999.828056	11.142810	-0.060540	4.815375
300.627141	7999.853104	11.147815	-0.060558	4.815382
300.404547	7999.830176	11.152819	-0.060516	4.815376
300.648765	7999.841667	11.157824	-0.060561	4.815379
300.517568	7999.948482	11.162829	-0.060537	4.815410
300.563539	7999.833810	11.167834	-0.060545	4.815377
300.719493	7999.816060	11.172839	-0.060574	4.815371
300.479699	7999.924288	11.177843	-0.060529	4.815404
300.472805	7999.838665	11.182848	-0.060527	4.815379
300.422305	7999.966047	11.187853	-0.060518	4.815416
300.419872	7999.818517	11.192858	-0.060517	4.815373
300.542159	7999.868603	11.197863	-0.060540	4.815387
300.366532	7999.959724	11.202867	-0.060507	4.815414
300.657317	7999.810622	11.207872	-0.060561	4.815370
300.773178	7999.922583	11.212877	-0.060582	4.815402
300.834677	7999.937470	11.217882	-0.060593	4.815406
300.488332	7999.956313	11.222887	-0.060529	4.815413
300.659824	7999.930270	11.227891	-0.060560	4.815404
300.876251	7999.783146	11.232896	-0.060600	4.815360
300.618863	7999.835516	11.237901	-0.060552	4.815377
300.558405	7999.821675	11.242906	-0.060541	4.815373
300.834609	7999.945900	11.247911	-0.060592	4.815408
300.577738	7999.948053	11.252915	-0.060544	4.815410
300.481540	7999.823554	11.257920	-0.060526	4.815374
300.485193	7999.973202	11.262925	-0.060526	4.815418
300.523922	7999.831694	11.267930	-0.060533	4.815376
300.664480	7999.893837	11.272935	-0.060559	4.815394
300.542511	7999.744335	11.277939	-0.060536	4.815351
300.595642	7999.799692	11.282944	-0.060546	4.815367
300.675834	7999.810613	11.287949	-0.060561	4.815370
300.540580	7999.953694	11.292954	-0.060535	4.815412
300.795445	7999.737744	11.297959	-0.060582	4.815348
300.620907	7999.936814	11.302963	-0.060550	4.815407
300.739414	7999.846848	11.307968	-0.060572	4.815380
300.646385	7999.804686	11.312973	-0.060554	4.815368
300.580534	7999.961736	11.317978	-0.060542	4.815414
300.703401	7999.778872	11.322983	-0.060564	4.815360
300.659106	7999.884983	11.327987	-0.060556	4.815391
300.686549	7999.846946	11.332992	-0.060561	4.815380
300.494103	7999.930309	11.337997	-0.060525	4.815405
300.714381	7999.835611	11.343002	-0.060565	4.815377
300.760218	7999.856652	11.348007	-0.060574	4.815383
300.579239	7999.919900	11.353011	-0.060540	4.815402
300.584138	7999.743639	11.358016	-0.060540	4.815350
300.535258	7999.857155	11.363021	-0.060531	4.815384
300.628852	7999.736858	11.368026	-0.060548	4.815348
300.580220	7999.847172	11.373031	-0.060539	4.815381
300.704730	7999.950726	11.378035	-0.060562	4.815410
300.646419	7999.914479	11.383040	-0.060551	4.815400
300.468277	7999.826030	11.388045	-0.060517	4.815375
300.566388	7999.814806	11.393050	-0.060536	4.815371
300.966099	7999.861991	11.398055	-0.060610	4.815383
300.752086	7999.924694	11.403059	-0.060570	4.815403
300.744968	7999.865782	11.408064	-0.060568	4.815385
300.715096	7999.833211	11.413069	-0.060562	4.815376
300.884092	7999.816745	11.418074	-0.060594	4.815370
300.811568	7999.851862	11.423079	-0.060580	4.815381
300.689734	7999.850900	11.428083	-0.060557	4.815381
300.830100	7999.743129	11.433088	-0.060583	4.815349
300.888126	7999.859478	11.438093	-0.060593	4.815383
300.702454	7999.961120	11.443098	-0.060559	4.815414
300.772605	7999.734641	11.448103	-0.060571	4.815347
300.687683	7999.913817	11.453107	-0.060556	4.815400
300.686601	7999.747075	11.458112	-0.060555	4.815351
300.568753	7999.902197	11.463117	-0.060533	4.815397
300.730189	7999.852479	11.468122	-0.060563	4.815382
300.724257	7999.836332	11.473127	-0.060561	4.815377
300.684094	7999.817483	11.478131	-0.060554	4.815372
300.708828	7999.849931	11.483136	-0.060558	4.815381
300.865316	7999.814023	11.488141	-0.060587	4.815370
300.649829	7999.953643	11.493146	-0.060547	4.815412
300.733700	7999.849213	11.498151	-0.060562	4.815381
300.589707	7999.816896	11.503155	-0.060535	4.815372
300.681613	7999.946628	11.508160	-0.060552	4.815409
300.847644	7999.818976	11.513165	-0.060583	4.815371
300.878175	7999.849382	11.518170	-0.060588	4.815380
300.733823	7999.777520	11.523175	-0.060561	4.815360
300.707682	7999.839049	11.528179	-0.060556	4.815378
300.828659	7999.769428	11.533184	-0.060578	4.815357
300.716339	7999.834878	11.538189	-0.060557	4.815377
300.699764	7999.835653	11.543194	-0.060554	4.815377
300.917436	7999.759079	11.548199	-0.060594	4.815354
300.822163	7999.841908	11.553203	-0.060576	4.815378
300.747225	7999.758368	11.558208	-0.060562	4.815354
300.757554	7999.894234	11.563213	-0.060564	4.815394
300.835598	7999.762993	11.568218	-0.060578	4.815355
300.863190	7999.757017	11.573223	-0.060583	4.815353
300.682276	7999.921786	11.578227	-0.060549	4.815402
300.740762	7999.809457	11.583232	-0.060560	4.815369
300.632064	7999.947633	11.588237	-0.060539	4.815410
300.675154	7999.885276	11.593242	-0.060547	4.815392
300.819573	7999.832071	11.598247	-0.060574	4.815375
300.956751	7999.826835	11.603251	-0.060599	4.815373
300.799888	7999.841325	11.608256	-0.060570	4.815378
300.757352	7999.849152	11.613261	-0.060561	4.815381
301.009470	7999.826578	11.618266	-0.060608	4.815373
300.812818	7999.839342	11.623271	-0.060571	4.815378
300.819551	7999.827679	11.628275	-0.060572	4.815374
300.833124	7999.815059	11.633280	-0.060575	4.815370
300.835662	7999.856758	11.638285	-0.060575	4.815383
300.669230	7999.865747	11.643290	-0.060544	4.815386
300.766210	7999.773289	11.648295	-0.060561	4.815359
300.783534	7999.819506	11.653299	-0.060564	4.815372
300.814476	7999.852055	11.658304	-0.060570	4.815381
300.767643	7999.740126	11.663309	-0.060561	4.815349
300.964438	7999.872658	11.668314	-0.060598	4.815387
300.974396	7999.732812	11.673319	-0.060599	4.815346
300.748969	7999.927837	11.678323	-0.060557	4.815404
300.963378	7999.765719	11.683328	-0.060597	4.815355
300.850639	7999.808721	11.688333	-0.060575	4.815369
300.817477	7999.832732	11.693338	-0.060569	4.815376
300.822343	7999.845616	11.698343	-0.060570	4.815380
300.804023	7999.828196	11.703347	-0.060566	4.815375
300.949779	7999.827376	11.708352	-0.060593	4.815374
300.900739	7999.949439	11.713357	-0.060584	4.815409
300.996563	7999.835589	11.718362	-0.060601	4.815376
301.138695	7999.836847	11.723367	-0.060627	4.815375
300.926108	7999.814083	11.728371	-0.060588	4.815370
301.096522	7999.848935	11.733376	-0.060619	4.815379
300.791932	7999.824653	11.738381	-0.060562	4.815374
300.747891	7999.940387	11.743386	-0.060554	4.815408
300.888823	7999.813390	11.748391	-0.060580	4.815370
300.922168	7999.960322	11.753395	-0.060586	4.815413
301.096713	7999.877693	11.758400	-0.060618	4.815388
301.039563	7999.816887	11.763405	-0.060607	4.815370
300.877577	7999.813125	11.768410	-0.060577	4.815370
300.979456	7999.862875	11.773415	-0.060596	4.815384
300.765597	7999.836885	11.778419	-0.060556	4.815377
300.966130	7999.844449	11.783424	-0.060593	4.815379
301.081489	7999.830304	11.788429	-0.060614	4.815374
301.149822	7999.838893	11.793434	-0.060626	4.815376
301.233846	7999.847740	11.798439	-0.060642	4.815378
301.073810	7999.818364	11.803443	-0.060612	4.815370
300.950138	7999.863323	11.808448	-0.060589	4.815384
300.890413	7999.767210	11.813453	-0.060577	4.815356
300.879721	7999.928376	11.818458	-0.060575	4.815404
300.987106	7999.775178	11.823463	-0.060595	4.815358
300.784979	7999.907538	11.828467	-0.060557	4.815398
300.973375	7999.789873	11.833472	-0.060592	4.815363
301.062991	7999.900332	11.838477	-0.060608	4.815395
301.124864	7999.823324	11.843482	-0.060620	4.815372
301.123797	7999.809394	11.848487	-0.060619	4.815368
301.048919	7999.940649	11.853491	-0.060605	4.815406
300.999796	7999.846848	11.858496	-0.060596	4.815379
301.065824	7999.960124	11.863501	-0.060608	4.815412
301.098240	7999.863394	11.868506	-0.060614	4.815384
301.179866	7999.824114	11.873511	-0.060628	4.815372
301.156989	7999.851501	11.878515	-0.060624	4.815380
301.041049	7999.820715	11.883520	-0.060602	4.815371
301.202605	7999.826567	11.888525	-0.060632	4.815372
301.080307	7999.845902	11.893530	-0.060609	4.815379
301.114819	7999.824010	11.898535	-0.060615	4.815372
300.946849	7999.943042	11.903539	-0.060584	4.815408
301.038429	7999.836603	11.908544	-0.060601	4.815376
300.974479	7999.832322	11.913549	-0.060588	4.815375
300.921434	7999.938289	11.918554	-0.060578	4.815406
301.171228	7999.726530	11.923559	-0.060625	4.815343
300.855456	7999.947847	11.928563	-0.060566	4.815409
300.966972	7999.737012	11.933568	-0.060586	4.815347
301.155293	7999.842688	11.938573	-0.060621	4.815377
301.162142	7999.925066	11.943578	-0.060622	4.815401
300.976904	7999.730705	11.948583	-0.060587	4.815345
300.983064	7999.949855	11.953587	-0.060588	4.815409
301.212013	7999.735614	11.958592	-0.060631	4.815346
301.192590	7999.883813	11.963597	-0.060627	4.815389
301.145642	7999.760127	11.968602	-0.060618	4.815353
301.170476	7999.838527	11.973607	-0.060622	4.815376
300.973734	7999.839534	11.978611	-0.060585	4.815377
301.081748	7999.850915	11.983616	-0.060605	4.815380
300.875822	7999.841085	11.988621	-0.060567	4.815378
301.151940	7999.840279	11.993626	-0.060618	4.815377
301.261671	7999.750169	11.998631	-0.060638	4.815350
301.158512	7999.825388	12.003635	-0.060619	4.815372
301.064791	7999.823821	12.008640	-0.060601	4.815372
300.888711	7999.819827	12.013645	-0.060568	4.815372
300.919979	7999.961382	12.018650	-0.060574	4.815413
301.005650	7999.844159	12.023655	-0.060589	4.815379
301.208200	7999.814355	12.028659	-0.060627	4.815369
300.955460	7999.856115	12.033664	-0.060580	4.815382
301.118068	7999.801073	12.038669	-0.060610	4.815365
301.079985	7999.846376	12.043674	-0.060602	4.815379
300.952523	7999.851733	12.048679	-0.060578	4.815381
300.980613	7999.815844	12.053683	-0.060583	4.815370
301.100142	7999.838100	12.058688	-0.060605	4.815376
301.206063	7999.878300	12.063693	-0.060625	4.815388
301.018205	7999.721298	12.068698	-0.060590	4.815343
301.198316	7999.867446	12.073703	-0.060623	4.815385
301.032483	7999.825150	12.078707	-0.060592	4.815373
300.965730	7999.865706	12.083712	-0.060579	4.815385
301.004130	7999.758389	12.088717	-0.060586	4.815354
301.054208	7999.840411	12.093722	-0.060595	4.815377
300.997162	7999.749685	12.098727	-0.060584	4.815351
300.971283	7999.848621	12.103731	-0.060579	4.815380
300.951512	7999.864304	12.108736	-0.060576	4.815385
301.067459	7999.764679	12.113741	-0.060597	4.815355
301.015796	7999.947610	12.118746	-0.060587	4.815409
301.220958	7999.755418	12.123751	-0.060625	4.815352
301.022517	7999.830133	12.128755	-0.060588	4.815375
300.972571	7999.934014	12.133760	-0.060578	4.815405
301.121724	7999.793260	12.138765	-0.060606	4.815363
301.108918	7999.750284	12.143770	-0.060603	4.815351
301.128622	7999.849972	12.148775	-0.060607	4.815380
301.011825	7999.824515	12.153779	-0.060585	4.815373
301.133412	7999.864972	12.158784	-0.060607	4.815384
300.953642	7999.747643	12.163789	-0.060573	4.815351
301.005920	7999.852143	12.168794	-0.060583	4.815381
301.367200	7999.764046	12.173799	-0.060650	4.815354
301.188302	7999.824123	12.178803	-0.060617	4.815372
301.060723	7999.862606	12.183808	-0.060593	4.815384
301.229187	7999.833308	12.188813	-0.060624	4.815375
301.221052	7999.833154	12.193818	-0.060622	4.815375
301.166390	7999.877115	12.198823	-0.060612	4.815388
300.991848	7999.740636	12.203827	-0.060579	4.815349
301.227515	7999.949683	12.208832	-0.060623	4.815409
301.254288	7999.878506	12.213837	-0.060627	4.815388
301.196996	7999.925630	12.218842	-0.060616	4.815402
301.232346	7999.746664	12.223847	-0.060623	4.815349
301.306371	7999.857934	12.228851	-0.060636	4.815381
301.291637	7999.871564	12.233856	-0.060633	4.815385
301.227282	7999.713394	12.238861	-0.060621	4.815340
301.125972	7999.956418	12.243866	-0.060602	4.815411
301.309709	7999.762803	12.248871	-0.060636	4.815354
301.110868	7999.944375	12.253875	-0.060599	4.815408
301.060199	7999.835587	12.258880	-0.060589	4.815376
301.102432	7999.845882	12.263885	-0.060597	4.815379
301.055608	7999.963707	12.268890	-0.060588	4.815414
301.109756	7999.848101	12.273895	-0.060598	4.815380
301.242832	7999.817150	12.278899	-0.060622	4.815370
301.321067	7999.743618	12.283904	-0.060637	4.815348
301.245456	7999.874860	12.288909	-0.060622	4.815387
301.317774	7999.740318	12.293914	-0.060636	4.815347
301.377578	7999.857766	12.298919	-0.060646	4.815381
301.247754	7999.834231	12.303923	-0.060622	4.815375
301.329364	7999.844107	12.308928	-0.060637	4.815377
301.605816	7999.785601	12.313933	-0.060688	4.815359
301.412902	7999.763162	12.318938	-0.060652	4.815353
301.379823	7999.801067	12.323943	-0.060646	4.815365
301.216235	7999.775907	12.328947	-0.060615	4.815358
301.403281	7999.804621	12.333952	-0.060650	4.815365
301.367616	7999.915151	12.338957	-0.060643	4.815398
301.445356	7999.750776	12.343962	-0.060657	4.815350
301.458874	7999.761666	12.348967	-0.060659	4.815353
301.096231	7999.833671	12.353971	-0.060592	4.815375
301.154864	7999.844237	12.358976	-0.060602	4.815378
301.372451	7999.739877	12.363981	-0.060643	4.815347
301.339637	7999.836561	12.368986	-0.060636	4.815375
301.337317	7999.769179	12.373991	-0.060636	4.815355
301.260418	7999.841626	12.378995	-0.060621	4.815377
301.438410	7999.739818	12.384000	-0.060654	4.815346
301.288445	7999.871971	12.389005	-0.060626	4.815386
301.265740	7999.842723	12.394010	-0.060621	4.815377
301.443627	7999.740914	12.399015	-0.060654	4.815347
301.415881	7999.841956	12.404019	-0.060649	4.815376
301.351852	7999.725468	12.409024	-0.060637	4.815343
301.392338	7999.913127	12.414029	-0.060644	4.815397
301.308100	7999.754628	12.419034	-0.060628	4.815351
301.260856	7999.879927	12.424039	-0.060619	4.815388
301.299002	7999.830311	12.429043	-0.060626	4.815374
301.238360	7999.749144	12.434048	-0.060615	4.815350
301.287525	7999.822602	12.439053	-0.060624	4.815371
301.330704	7999.764521	12.444058	-0.060631	4.815354
301.540137	7999.871615	12.449063	-0.060670	4.815385
301.480340	7999.735961	12.454067	-0.060659	4.815345
301.470876	7999.830893	12.459072	-0.060657	4.815373
301.299725	7999.803470	12.464077	-0.060625	4.815366
301.316794	7999.742820	12.469082	-0.060628	4.815348
301.266013	7999.845620	12.474087	-0.060618	4.815378
301.323422	7999.831587	12.479091	-0.060628	4.815374
301.620546	7999.862119	12.484096	-0.060684	4.815381
301.324803	7999.757835	12.489101	-0.060628	4.815352
301.340921	7999.833954	12.494106	-0.060631	4.815375
301.598518	7999.840323	12.499111	-0.060679	4.815375
301.311401	7999.726565	12.504115	-0.060625	4.815343
301.247904	7999.824879	12.509120	-0.060613	4.815372
301.422812	7999.750805	12.514125	-0.060645	4.815350
301.228238	7999.828790	12.519130	-0.060609	4.815374
301.123136	7999.747958	12.524135	-0.060589	4.815350
301.403008	7999.827361	12.529139	-0.060641	4.815372
301.430515	7999.868403	12.534144	-0.060646	4.815384
301.221314	7999.746313	12.539149	-0.060607	4.815350
301.263674	7999.817522	12.544154	-0.060614	4.815370
301.396040	7999.862432	12.549159	-0.060639	4.815383
301.212078	7999.827317	12.554163	-0.060604	4.815373
301.157678	7999.863802	12.559168	-0.060594	4.815384
301.383192	7999.822621	12.564173	-0.060636	4.815371
301.416582	7999.829565	12.569178	-0.060642	4.815373
301.382960	7999.850363	12.574183	-0.060635	4.815379
301.182266	7999.962443	12.579187	-0.060598	4.815413
301.354151	7999.824201	12.584192	-0.060629	4.815372
301.309152	7999.854429	12.589197	-0.060621	4.815381
301.198702	7999.722214	12.594202	-0.060600	4.815343
301.408019	7999.825031	12.599207	-0.060639	4.815372
301.481104	7999.830492	12.604211	-0.060652	4.815373
301.463927	7999.853699	12.609216	-0.060649	4.815380
301.352265	7999.835807	12.614221	-0.060628	4.815375
301.410467	7999.834611	12.619226	-0.060638	4.815375
301.381758	7999.761450	12.624231	-0.060633	4.815353
301.555092	7999.748262	12.629235	-0.060665	4.815349
301.559691	7999.859456	12.634240	-0.060666	4.815381
301.610461	7999.811117	12.639245	-0.060675	4.815367
301.521399	7999.952825	12.644250	-0.060658	4.815409
301.675443	7999.724522	12.649255	-0.060686	4.815341
301.503069	7999.829590	12.654259	-0.060654	4.815373
301.580570	7999.808408	12.659264	-0.060668	4.815366
301.545103	7999.862303	12.664269	-0.060662	4.815382
301.676312	7999.833459	12.669274	-0.060686	4.815373
301.666387	7999.865335	12.674279	-0.060684	4.815382
301.650216	7999.847950	12.679283	-0.060680	4.815377
301.694264	7999.751411	12.684288	-0.060688	4.815349
301.572760	7999.888309	12.689293	-0.060666	4.815390
301.456502	7999.933390	12.694298	-0.060644	4.815403
301.543026	7999.841827	12.699303	-0.060660	4.815376
301.520838	7999.822206	12.704307	-0.060655	4.815370
301.450477	7999.830643	12.709312	-0.060642	4.815373
301.585121	7999.778345	12.714317	-0.060667	4.815357
301.284715	7999.868476	12.719322	-0.060611	4.815385
301.595465	7999.756035	12.724327	-0.060668	4.815351
301.554343	7999.816249	12.729331	-0.060660	4.815369
301.551024	7999.809763	12.734336	-0.060659	4.815367
301.570866	7999.839992	12.739341	-0.060663	4.815375
301.345884	7999.840534	12.744346	-0.060621	4.815377
301.559702	7999.764965	12.749351	-0.060660	4.815354
301.521698	7999.810269	12.754355	-0.060653	4.815367
301.468766	7999.846778	12.759360	-0.060643	4.815378
301.573490	7999.847418	12.764365	-0.060662	4.815378
301.406399	7999.827542	12.769370	-0.060631	4.815373
301.470989	7999.760196	12.774375	-0.060643	4.815353
301.466603	7999.841320	12.779379	-0.060642	4.815376
301.588893	7999.860417	12.784384	-0.060664	4.815381
301.734630	7999.760214	12.789389	-0.060691	4.815351
301.537222	7999.854182	12.794394	-0.060654	4.815380
301.389943	7999.772653	12.799399	-0.060627	4.815357
301.519910	7999.829278	12.804403	-0.060651	4.815373
301.432783	7999.829958	12.809408	-0.060634	4.815373
301.501239	7999.840686	12.814413	-0.060647	4.815376
301.456895	7999.826042	12.819418	-0.060638	4.815372
301.670283	7999.820995	12.824423	-0.060678	4.815370
301.601607	7999.872205	12.829427	-0.060665	4.815385
301.598713	7999.736422	12.834432	-0.060664	4.815345
301.529981	7999.878464	12.839437	-0.060651	4.815387
301.221599	7999.769698	12.844442	-0.060593	4.815357
301.421451	7999.784731	12.849447	-0.060630	4.815360
301.458029	7999.876149	12.854451	-0.060637	4.815387
301.221086	7999.791003	12.859456	-0.060592	4.815363
301.346146	7999.804802	12.864461	-0.060616	4.815366
301.412413	7999.744964	12.869466	-0.060628	4.815349
301.573209	7999.892933	12.874471	-0.060657	4.815391
301.507691	7999.752909	12.879475	-0.060645	4.815350
301.488534	7999.855162	12.884480	-0.060641	4.815380
301.561746	7999.742007	12.889485	-0.060655	4.815347
301.536496	7999.840953	12.894490	-0.060650	4.815376
301.519094	7999.733784	12.899495	-0.060646	4.815345
301.550287	7999.851828	12.904499	-0.060652	4.815379
301.469474	7999.860092	12.909504	-0.060637	4.815382
301.572378	7999.796585	12.914509	-0.060655	4.815363
301.444362	7999.735678	12.919514	-0.060631	4.815346
301.554497	7999.874260	12.924519	-0.060652	4.815386
301.585690	7999.827736	12.929523	-0.060657	4.815372
301.568468	7999.841324	12.934528	-0.060654	4.815376
301.711959	7999.851153	12.939533	-0.060680	4.815378
301.583059	7999.810535	12.944538	-0.060656	4.815367
301.518372	7999.762428	12.949543	-0.060644	4.815353
301.624155	7999.797282	12.954547	-0.060663	4.815363
301.491565	7999.815378	12.959552	-0.060638	4.815369
301.467064	7999.857699	12.964557	-0.060634	4.815381
301.468560	7999.792518	12.969562	-0.060634	4.815362
301.664258	7999.774355	12.974567	-0.060670	4.815356
301.622033	7999.775776	12.979571	-0.060662	4.815357
301.616165	7999.891072	12.984576	-0.060661	4.815390
301.861632	7999.755113	12.989581	-0.060706	4.815350
301.689138	7999.737285	12.994586	-0.060674	4.815345
301.616000	7999.895285	12.999591	-0.060660	4.815392
301.685927	7999.792762	13.004595	-0.060673	4.815361
301.797252	7999.741148	13.009600	-0.060693	4.815346
301.578505	7999.936284	13.014605	-0.060652	4.815404
301.514981	7999.735382	13.019610	-0.060640	4.815345
301.774053	7999.792001	13.024615	-0.060688	4.815361
301.700047	7999.853809	13.029619	-0.060674	4.815379
301.469066	7999.757006	13.034624	-0.060631	4.815352
301.535389	7999.793346	13.039629	-0.060643	4.815362
301.458887	7999.872211	13.044634	-0.060629	4.815386
301.596420	7999.780422	13.049639	-0.060654	4.815358
301.716270	7999.837949	13.054643	-0.060676	4.815375
301.692420	7999.836467	13.059648	-0.060671	4.815374
301.731311	7999.813579	13.064653	-0.060678	4.815367
301.589882	7999.804814	13.069658	-0.060652	4.815365
301.868799	7999.782682	13.074663	-0.060704	4.815358
301.566417	7999.763779	13.079667	-0.060647	4.815354
301.438749	7999.760584	13.084672	-0.060623	4.815353
301.519072	7999.771508	13.089677	-0.060638	4.815356
301.484713	7999.823284	13.094682	-0.060631	4.815371
301.621543	7999.887503	13.099687	-0.060656	4.815390
301.529176	7999.745968	13.104691	-0.060639	4.815349
301.552241	7999.821133	13.109696	-0.060643	4.815370
301.440276	7999.897276	13.114701	-0.060622	4.815393
301.534435	7999.862477	13.119706	-0.060639	4.815383
301.673124	7999.777118	13.124711	-0.060665	4.815357
301.652455	7999.757522	13.129715	-0.060661	4.815351
301.462887	7999.871923	13.134720	-0.060625	4.815386
301.569935	7999.829857	13.139725	-0.060645	4.815373
301.581753	7999.742404	13.144730	-0.060647	4.815347
301.635816	7999.763581	13.149735	-0.060657	4.815353
301.728123	7999.764016	13.154739	-0.060674	4.815353
301.649016	7999.898407	13.159744	-0.060659	4.815393
301.513889	7999.833108	13.164749	-0.060634	4.815374
301.460844	7999.767026	13.169754	-0.060623	4.815355
301.753781	7999.803900	13.174759	-0.060678	4.815365
301.606772	7999.847406	13.179763	-0.060650	4.815378
301.664681	7999.742547	13.184768	-0.060661	4.815347
301.800295	7999.839874	13.189773	-0.060686	4.815375
301.806833	7999.749129	13.194778	-0.060687	4.815348
301.842805	7999.901449	13.199783	-0.060693	4.815393
301.605585	7999.828052	13.204787	-0.060649	4.815372
301.654255	7999.803189	13.209792	-0.060658	4.815365
301.767280	7999.819996	13.214797	-0.060678	4.815369
301.738673	7999.762866	13.219802	-0.060673	4.815353
301.542200	7999.806624	13.224807	-0.060636	4.815366
301.559939	7999.913760	13.229811	-0.060639	4.815398
301.334834	7999.740113	13.234816	-0.060597	4.815348
301.523249	7999.804115	13.239821	-0.060632	4.815366
301.589699	7999.841525	13.244826	-0.060644	4.815376
301.694755	7999.747063	13.249831	-0.060663	4.815348
301.597666	7999.802078	13.254835	-0.060645	4.815365
301.646153	7999.896899	13.259840	-0.060654	4.815392
301.704583	7999.823039	13.264845	-0.060665	4.815370
301.451919	7999.768624	13.269850	-0.060617	4.815356
301.588969	7999.837121	13.274855	-0.060643	4.815375
301.733209	7999.805286	13.279859	-0.060669	4.815365
301.676141	7999.795775	13.284864	-0.060658	4.815363
301.661838	7999.933373	13.289869	-0.060656	4.815403
301.580579	7999.784541	13.294874	-0.060640	4.815360
301.660041	7999.824303	13.299879	-0.060655	4.815371
301.563656	7999.850477	13.304883	-0.060637	4.815379
301.616888	7999.824621	13.309888	-0.060646	4.815371
301.685471	7999.836419	13.314893	-0.060659	4.815375
301.586982	7999.887137	13.319898	-0.060640	4.815390
301.559479	7999.813996	13.324903	-0.060635	4.815369
301.554565	7999.761533	13.329907	-0.060634	4.815353
301.444086	7999.847317	13.334912	-0.060613	4.815379
301.700949	7999.808792	13.339917	-0.060661	4.815366
301.737700	7999.768771	13.344922	-0.060667	4.815355
301.745462	7999.777428	13.349927	-0.060668	4.815357
301.668413	7999.944982	13.354931	-0.060654	4.815406
301.708782	7999.761823	13.359936	-0.060661	4.815353
301.763028	7999.805444	13.364941	-0.060671	4.815365
301.509514	7999.746740	13.369946	-0.060624	4.815349
301.594082	7999.884901	13.374951	-0.060639	4.815389
301.981424	7999.790823	13.379955	-0.060711	4.815360
301.914581	7999.729856	13.384960	-0.060698	4.815342
301.829374	7999.915442	13.389965	-0.060682	4.815397
301.856349	7999.823965	13.394970	-0.060687	4.815370
301.940040	7999.785787	13.399975	-0.060702	4.815359
301.696631	7999.834113	13.404979	-0.060657	4.815374
301.868905	7999.809152	13.409984	-0.060689	4.815366
301.978378	7999.845136	13.414989	-0.060709	4.815376
301.807552	7999.777110	13.419994	-0.060677	4.815357
301.832125	7999.788182	13.424999	-0.060681	4.815360
301.734987	7999.849608	13.430003	-0.060663	4.815378
301.814277	7999.818838	13.435008	-0.060677	4.815369
301.830837	7999.798788	13.440013	-0.060680	4.815363
301.817918	7999.765427	13.445018	-0.060678	4.815353
301.685931	7999.783533	13.450023	-0.060653	4.815359
301.704647	7999.806264	13.455027	-0.060656	4.815366
301.852109	7999.894169	13.460032	-0.060683	4.815391
302.002127	7999.820753	13.465037	-0.060711	4.815369
301.910318	7999.774335	13.470042	-0.060694	4.815355
301.766565	7999.763393	13.475047	-0.060667	4.815353
301.792448	7999.811889	13.480051	-0.060671	4.815367
301.746656	7999.784398	13.485056	-0.060663	4.815359
301.765697	7999.848811	13.490061	-0.060666	4.815378
301.780670	7999.840489	13.495066	-0.060669	4.815375
301.824539	7999.802723	13.500071	-0.060677	4.815364
301.865653	7999.795901	13.505075	-0.060684	4.815362
301.728797	7999.850261	13.510080	-0.060658	4.815379
301.716230	7999.828661	13.515085	-0.060656	4.815372
301.576474	7999.768628	13.520090	-0.060629	4.815355
301.653526	7999.763469	13.525095	-0.060644	4.815354
301.858101	7999.761482	13.530099	-0.060681	4.815352
301.715860	7999.857429	13.535104	-0.060655	4.815381
301.624227	7999.753309	13.540109	-0.060637	4.815351
301.641412	7999.861504	13.545114	-0.060640	4.815382
301.818162	7999.755401	13.550119	-0.060673	4.815350
301.893336	7999.867761	13.555123	-0.060687	4.815383
301.670696	7999.850174	13.560128	-0.060645	4.815379
301.837978	7999.777042	13.565133	-0.060676	4.815357
301.677534	7999.841698	13.570138	-0.060646	4.815376
301.765405	7999.776874	13.575143	-0.060662	4.815357
301.850036	7999.822065	13.580147	-0.060678	4.815370
301.752423	7999.892033	13.585152	-0.060659	4.815391
301.742824	7999.778579	13.590157	-0.060657	4.815358
301.805295	7999.755012	13.595162	-0.060669	4.815350
301.756693	7999.856779	13.600167	-0.060659	4.815380
301.862715	7999.800803	13.605171	-0.060679	4.815364
301.870919	7999.750693	13.610176	-0.060680	4.815349
301.944416	7999.788220	13.615181	-0.060694	4.815360
301.909978	7999.847476	13.620186	-0.060687	4.815377
301.845309	7999.741663	13.625191	-0.060675	4.815346
302.015031	7999.757268	13.630195	-0.060706	4.815350
301.899080	7999.826933	13.635200	-0.060684	4.815371
301.816471	7999.809520	13.640205	-0.060669	4.815366
301.848393	7999.771557	13.645210	-0.060674	4.815355
302.137688	7999.785930	13.650215	-0.060728	4.815358
302.046164	7999.792948	13.655219	-0.060711	4.815360
301.738778	7999.833806	13.660224	-0.060653	4.815374
301.955190	7999.765760	13.665229	-0.060693	4.815353
301.956463	7999.764693	13.670234	-0.060694	4.815353
302.006603	7999.858473	13.675239	-0.060703	4.815380
301.889863	7999.802025	13.680243	-0.060681	4.815364
301.877999	7999.781506	13.685248	-0.060678	4.815358
301.832623	7999.822414	13.690253	-0.060670	4.815370
301.928597	7999.778027	13.695258	-0.060687	4.815357
302.120159	7999.803611	13.700263	-0.060723	4.815363
302.080314	7999.865983	13.705267	-0.060715	4.815382
301.875552	7999.740759	13.710272	-0.060677	4.815346
302.112562	7999.775642	13.715277	-0.060721	4.815355
302.023744	7999.847892	13.720282	-0.060704	4.815377
302.044151	7999.754169	13.725287	-0.060707	4.815349
301.986215	7999.895322	13.730291	-0.060696	4.815391
302.018875	7999.788978	13.735296	-0.060702	4.815360
301.895450	7999.800813	13.740301	-0.060679	4.815364
301.913283	7999.754068	13.745306	-0.060682	4.815350
301.870593	7999.760824	13.750311	-0.060674	4.815352
301.926658	7999.793789	13.755315	-0.060684	4.815361
301.862708	7999.849351	13.760320	-0.060672	4.815378
301.971649	7999.782737	13.765325	-0.060692	4.815358
302.086306	7999.849797	13.770330	-0.060713	4.815377
301.877925	7999.830308	13.775335	-0.060674	4.815372
301.714056	7999.773084	13.780339	-0.060644	4.815356
301.929768	7999.755252	13.785344	-0.060683	4.815350
302.003475	7999.912470	13.790349	-0.060697	4.815396
301.870373	7999.777742	13.795354	-0.060672	4.815357
302.024522	7999.811257	13.800359	-0.060700	4.815366
302.023819	7999.783441	13.805363	-0.060700	4.815358
301.902441	7999.749359	13.810368	-0.060677	4.815349
301.958140	7999.857122	13.815373	-0.060687	4.815380
302.007779	7999.764951	13.820378	-0.060696	4.815353
301.919103	7999.833997	13.825383	-0.060680	4.815373
301.967522	7999.880728	13.830387	-0.060689	4.815387
301.917366	7999.812557	13.835392	-0.060679	4.815367
301.660087	7999.893781	13.840397	-0.060631	4.815392
301.621477	7999.768095	13.845402	-0.060623	4.815355
301.642756	7999.806897	13.850407	-0.060627	4.815367
301.752431	7999.815099	13.855411	-0.060647	4.815369
301.699057	7999.843051	13.860416	-0.060637	4.815377
301.916438	7999.775021	13.865421	-0.060677	4.815356
301.874703	7999.830950	13.870426	-0.060669	4.815373
301.794690	7999.745188	13.875431	-0.060654	4.815348
301.783841	7999.764225	13.880435	-0.060652	4.815354
301.911255	7999.846456	13.885440	-0.060676	4.815377
302.199742	7999.762501	13.890445	-0.060729	4.815351
301.910057	7999.835710	13.895450	-0.060675	4.815374
301.900514	7999.743631	13.900455	-0.060673	4.815347
301.945603	7999.783895	13.905459	-0.060681	4.815359
301.889987	7999.853487	13.910464	-0.060671	4.815379
302.099127	7999.774634	13.915469	-0.060709	4.815355
302.046228	7999.868850	13.920474	-0.060699	4.815383
301.920921	7999.744938	13.925479	-0.060676	4.815347
301.865388	7999.895748	13.930483	-0.060665	4.815392
301.936550	7999.754774	13.935488	-0.060678	4.815350
301.837911	7999.795872	13.940493	-0.060659	4.815363
301.706201	7999.779786	13.945498	-0.060635	4.815359
301.743453	7999.873352	13.950503	-0.060642	4.815386
301.768321	7999.822449	13.955507	-0.060646	4.815371
301.705992	7999.781861	13.960512	-0.060634	4.815359
301.859015	7999.815357	13.965517	-0.060662	4.815368
302.069660	7999.763245	13.970522	-0.060701	4.815352
302.029283	7999.760422	13.975527	-0.060694	4.815351
301.952792	7999.918367	13.980531	-0.060679	4.815398
301.950857	7999.778324	13.985536	-0.060679	4.815357
301.793096	7999.809897	13.990541	-0.060649	4.815367
301.759037	7999.828550	13.995546	-0.060642	4.815373
301.690595	7999.782519	14.000551	-0.060629	4.815360
301.769231	7999.886385	14.005555	-0.060644	4.815390
301.761076	7999.764407	14.010560	-0.060642	4.815354
302.007124	7999.799439	14.015565	-0.060688	4.815363
301.844210	7999.791387	14.020570	-0.060657	4.815361
301.825902	7999.897929	14.025575	-0.060654	4.815393
301.862574	7999.820504	14.030579	-0.060660	4.815370
301.689723	7999.739622	14.035584	-0.060628	4.815347
302.037411	7999.769919	14.040589	-0.060692	4.815354
301.909889	7999.822295	14.045594	-0.060668	4.815370
302.036495	7999.828639	14.050599	-0.060692	4.815371
302.203147	7999.740536	14.055603	-0.060722	4.815345
301.902262	7999.952484	14.060608	-0.060666	4.815408
302.084700	7999.763121	14.065613	-0.060700	4.815352
301.989497	7999.728402	14.070618	-0.060682	4.815342
301.960745	7999.877517	14.075623	-0.060676	4.815386
301.929956	7999.800047	14.080627	-0.060670	4.815364
301.892887	7999.757739	14.085632	-0.060663	4.815351
301.969450	7999.795316	14.090637	-0.060677	4.815362
301.830730	7999.753468	14.095642	-0.060651	4.815350
301.915960	7999.874542	14.100647	-0.060667	4.815385
302.005635	7999.765933	14.105651	-0.060683	4.815353
301.914002	7999.833862	14.110656	-0.060666	4.815374
301.835094	7999.762010	14.115661	-0.060651	4.815353
301.744572	7999.819271	14.120666	-0.060634	4.815370
301.904613	7999.861433	14.125671	-0.060664	4.815382
301.952946	7999.745730	14.130675	-0.060672	4.815348
301.979603	7999.767523	14.135680	-0.060677	4.815354
301.991560	7999.760220	14.140685	-0.060679	4.815352
302.011746	7999.886633	14.145690	-0.060683	4.815389
301.986362	7999.799634	14.150695	-0.060678	4.815363
302.045301	7999.782421	14.155699	-0.060689	4.815358
302.004089	7999.853320	14.160704	-0.060681	4.815379
301.922179	7999.778212	14.165709	-0.060665	4.815357
301.847642	7999.759864	14.170714	-0.060651	4.815352
301.919680	7999.862554	14.175719	-0.060664	4.815382
301.851186	7999.801560	14.180723	-0.060651	4.815365
301.809503	7999.864970	14.185728	-0.060643	4.815383
302.060233	7999.804971	14.190733	-0.060690	4.815365
301.732032	7999.849760	14.195738	-0.060629	4.815379
301.778284	7999.774631	14.200743	-0.060637	4.815357
301.898992	7999.864232	14.205747	-0.060659	4.815383
301.775062	7999.848274	14.210752	-0.060636	4.815379
301.977204	7999.747933	14.215757	-0.060673	4.815348
301.890388	7999.809530	14.220762	-0.060657	4.815367
302.048826	7999.770449	14.225767	-0.060686	4.815355
301.857099	7999.805736	14.230771	-0.060650	4.815366
301.861279	7999.767314	14.235776	-0.060651	4.815355
302.084184	7999.797689	14.240781	-0.060692	4.815362
301.935147	7999.874289	14.245786	-0.060664	4.815385
302.047531	7999.759643	14.250791	-0.060685	4.815351
301.900275	7999.746507	14.255795	-0.060657	4.815348
301.924484	7999.532094	14.260800	-0.060661	4.815286
301.970564	7996.392471	14.265805	-0.060668	4.814368
301.896422	7990.759540	14.270810	-0.060650	4.812722
301.914516	7983.968458	14.275815	-0.060649	4.810736
301.751002	7976.744023	14.280819	-0.060613	4.808624
301.670571	7968.992950	14.285824	-0.060593	4.806356
301.984623	7961.215468	14.290829	-0.060646	4.804078
301.891265	7953.362840	14.295834	-0.060623	4.801778
301.707576	7945.330516	14.300839	-0.060584	4.799425
301.994627	7937.438081	14.305843	-0.060632	4.797110
301.819031	7929.421206	14.310848	-0.060594	4.794759
301.837145	7921.412233	14.315853	-0.060592	4.792408
301.771993	7913.367723	14.320858	-0.060574	4.790047
301.693753	7905.372715	14.325863	-0.060554	4.787698
301.617467	7897.388067	14.330867	-0.060534	4.785352
301.394849	7889.392613	14.335872	-0.060488	4.783002
301.509384	7881.395172	14.340877	-0.060503	4.780648
301.380487	7873.412146	14.345882	-0.060474	4.778299
301.297605	7865.365885	14.350887	-0.060453	4.775930
301.292844	7857.447558	14.355891	-0.060447	4.773597
301.288717	7849.318186	14.360896	-0.060441	4.771200
301.355466	7841.388526	14.365901	-0.060448	4.768861
301.126571	7833.337413	14.370906	-0.060400	4.766486
301.362209	7825.351088	14.375911	-0.060438	4.764127
301.390511	7817.440101	14.380915	-0.060438	4.761791
301.139547	7809.317383	14.385920	-0.060386	4.759391
301.220920	7801.438162	14.390925	-0.060395	4.757061
301.175489	7793.313368	14.395930	-0.060381	4.754658
301.085082	7785.291330	14.400935	-0.060359	4.752284
301.152994	7777.283537	14.405939	-0.060366	4.749912
301.111627	7769.337529	14.410944	-0.060353	4.747558
301.138033	7761.324611	14.415949	-0.060353	4.745183
300.884442	7753.375902	14.420954	-0.060300	4.742827
300.827625	7745.315467	14.425959	-0.060284	4.740435
301.037996	7737.332287	14.430963	-0.060318	4.738065
300.783899	7729.333694	14.435968	-0.060265	4.735690
300.681668	7721.336500	14.440973	-0.060241	4.733314
300.882317	7713.264384	14.445978	-0.060272	4.730913
300.868637	7705.304462	14.450983	-0.060264	4.728545
300.928654	7697.321950	14.455987	-0.060270	4.726170
300.813395	7689.289452	14.460992	-0.060243	4.723778
300.856864	7681.364097	14.465997	-0.060246	4.721417
300.766148	7673.303318	14.471002	-0.060224	4.719015
300.766813	7665.354213	14.476007	-0.060218	4.716644
300.787688	7657.356974	14.481011	-0.060217	4.714258
300.459405	7649.243882	14.486016	-0.060150	4.711837
300.476949	7641.270519	14.491021	-0.060148	4.709455
300.495324	7633.261507	14.496026	-0.060146	4.707062
300.420149	7625.221424	14.501031	-0.060127	4.704658
300.375246	7617.327614	14.506035	-0.060113	4.702297
300.407571	7609.285032	14.511040	-0.060113	4.699890
300.559074	7601.362045	14.516045	-0.060136	4.697517
300.318343	7593.294540	14.521050	-0.060086	4.695101
300.271348	7585.264825	14.526055	-0.060072	4.692694
300.399966	7577.263254	14.531059	-0.060090	4.690294
300.356898	7569.286539	14.536064	-0.060077	4.687901
300.288714	7561.307538	14.541069	-0.060059	4.685506
300.421904	7553.317171	14.546074	-0.060078	4.683106
300.231266	7545.286494	14.551079	-0.060037	4.680693
300.437160	7537.332735	14.556083	-0.060070	4.678301
300.295181	7529.217261	14.561088	-0.060038	4.675860
300.395089	7521.192313	14.566093	-0.060051	4.673444
300.251733	7513.185883	14.571098	-0.060019	4.671033
300.154812	7505.183860	14.576103	-0.059996	4.668623
300.253121	7497.218962	14.581107	-0.060009	4.666221
300.001856	7489.249441	14.586112	-0.059956	4.663818
299.919788	7481.240327	14.591117	-0.059936	4.661401
300.045275	7473.235153	14.596122	-0.059954	4.658984
299.923937	7465.240447	14.601127	-0.059925	4.656569
299.599411	7457.244096	14.606131	-0.059860	4.654153
299.619906	7449.175715	14.611136	-0.059858	4.651713
299.736656	7441.219143	14.616141	-0.059874	4.649306
299.670691	7433.212531	14.621146	-0.059857	4.646882
299.566802	7425.202819	14.626151	-0.059832	4.644456
299.624975	7417.267769	14.631155	-0.059837	4.642052
299.771611	7409.208329	14.636160	-0.059859	4.639608
299.684378	7401.245220	14.641165	-0.059837	4.637193
299.572525	7393.197817	14.646170	-0.059811	4.634750
299.489377	7385.175311	14.651175	-0.059790	4.632314
299.478760	7377.156143	14.656179	-0.059783	4.629878
299.574477	7369.160849	14.661184	-0.059795	4.627447
299.614747	7361.161461	14.666189	-0.059797	4.625014
299.453148	7353.239952	14.671194	-0.059762	4.622604
299.322891	7345.181198	14.676199	-0.059732	4.620150
299.386422	7337.220111	14.681203	-0.059738	4.617725
299.254478	7329.126941	14.686208	-0.059708	4.615259
299.176622	7321.209085	14.691213	-0.059688	4.612844
299.251612	7313.155250	14.696218	-0.059697	4.610387
299.181344	7305.180371	14.701223	-0.059678	4.607952
299.132744	7297.130026	14.706227	-0.059664	4.605493
299.081975	7289.183078	14.711232	-0.059649	4.603065
299.313970	7281.137000	14.716237	-0.059687	4.600604
298.980386	7273.183501	14.721242	-0.059619	4.598171
299.101025	7265.156271	14.726247	-0.059636	4.595714
299.109922	7257.100849	14.731251	-0.059633	4.593247
299.009048	7249.075408	14.736256	-0.059608	4.590788
299.025541	7241.087692	14.741261	-0.059606	4.588339
298.781580	7233.104780	14.746266	-0.059555	4.585890
298.865957	7225.123461	14.751271	-0.059565	4.583441
298.984425	7217.162565	14.756275	-0.059582	4.580996
298.888367	7209.116035	14.761280	-0.059559	4.578524
298.944416	7201.129309	14.766285	-0.059564	4.576069
298.722589	7193.132476	14.771290	-0.059517	4.573609
298.571859	7185.092143	14.776295	-0.059483	4.571134
298.637117	7177.146724	14.781299	-0.059490	4.568688
298.386205	7169.068901	14.786304	-0.059438	4.566199
298.457160	7161.104734	14.791309	-0.059446	4.563744
298.550209	7153.123492	14.796314	-0.059458	4.561283
298.436572	7145.091767	14.801319	-0.059431	4.558804
298.615701	7137.134955	14.806323	-0.059459	4.556348
298.246572	7129.127291	14.811328	-0.059385	4.553874
298.440780	7121.084081	14.816333	-0.059416	4.551388
298.322650	7113.108313	14.821338	-0.059388	4.548921
298.085927	7105.086095	14.826343	-0.059339	4.546439
298.399324	7097.128929	14.831347	-0.059392	4.543976
298.215157	7089.113228	14.836352	-0.059352	4.541492
298.235510	7081.122974	14.841357	-0.059350	4.539016
298.244506	7073.129097	14.846362	-0.059346	4.536537
298.171956	7065.087784	14.851367	-0.059327	4.534042
298.130579	7057.091959	14.856371	-0.059314	4.531560
298.028242	7049.057729	14.861376	-0.059290	4.529064
298.102462	7041.119187	14.866381	-0.059298	4.526597
298.056104	7033.094444	14.871386	-0.059284	4.524102
297.848209	7025.136496	14.876391	-0.059240	4.521625
298.155936	7017.130111	14.881395	-0.059292	4.519134
298.126618	7009.124539	14.886400	-0.059281	4.516640
297.923789	7001.066652	14.891405	-0.059238	4.514128
297.825744	6993.011513	14.896410	-0.059214	4.511616
297.887505	6985.039650	14.901415	-0.059220	4.509129
297.769352	6977.025663	14.906419	-0.059193	4.506627
297.656428	6969.022134	14.911424	-0.059166	4.504127
297.862053	6961.085265	14.916429	-0.059199	4.501648
297.880117	6953.075499	14.921434	-0.059197	4.499143
297.699334	6945.066004	14.926439	-0.059158	4.496637
297.892974	6937.072557	14.931443	-0.059188	4.494135
297.744764	6929.030909	14.936448	-0.059155	4.491616
297.695198	6921.069579	14.941453	-0.059141	4.489121
297.702207	6913.089255	14.946458	-0.059137	4.486619
297.603563	6905.003024	14.951463	-0.059113	4.484081
297.562998	6897.074937	14.956467	-0.059100	4.481592
297.550276	6889.020814	14.961472	-0.059092	4.479063
297.561581	6881.048465	14.966477	-0.059089	4.476557
297.331624	6873.031569	14.971482	-0.059040	4.474036
297.228154	6864.954416	14.976487	-0.059016	4.471494
297.458364	6856.984265	14.981491	-0.059053	4.468986
297.580752	6849.018741	14.986496	-0.059071	4.466477
297.468293	6841.039567	14.991501	-0.059044	4.463962
297.545368	6833.078554	14.996506	-0.059053	4.461452
297.422091	6825.001727	15.001511	-0.059025	4.458903
297.458409	6817.061109	15.006515	-0.059026	4.456397
297.243247	6808.993670	15.011520	-0.058980	4.453848
297.251832	6800.967645	15.016525	-0.058977	4.451311
297.233973	6793.049180	15.021530	-0.058968	4.448807
297.150453	6784.997939	15.026535	-0.058947	4.446259
297.105464	6776.986341	15.031539	-0.058933	4.443722
297.265647	6769.016028	15.036544	-0.058958	4.441198
297.180391	6761.079104	15.041549	-0.058936	4.438682
297.047031	6753.031250	15.046554	-0.058906	4.436129
297.070176	6744.954445	15.051559	-0.058905	4.433566
297.180943	6736.941040	15.056563	-0.058920	4.431023
297.059665	6728.936494	15.061568	-0.058892	4.428479
297.097200	6720.940199	15.066573	-0.058893	4.425937
297.091866	6712.983465	15.071578	-0.058887	4.423407
296.883935	6704.968591	15.076583	-0.058843	4.420855
296.843666	6697.030409	15.081587	-0.058830	4.418327
296.801953	6688.936159	15.086592	-0.058817	4.415748
296.728800	6680.969529	15.091597	-0.058798	4.413208
296.578737	6672.978391	15.096602	-0.058764	4.410658
296.621767	6664.976176	15.101607	-0.058767	4.408105
296.987645	6656.949967	15.106611	-0.058830	4.405543
296.499323	6648.999755	15.111616	-0.058733	4.403000
296.430308	6640.981083	15.116621	-0.058715	4.400436
296.601038	6633.013877	15.121626	-0.058741	4.397888
296.405441	6624.970595	15.126631	-0.058699	4.395313
296.630825	6616.979541	15.131635	-0.058736	4.392755
296.622826	6608.938632	15.136640	-0.058729	4.390178
296.598234	6600.982558	15.141645	-0.058719	4.387626
296.445157	6592.939026	15.146650	-0.058685	4.385045
296.535956	6584.971804	15.151655	-0.058697	4.382488
296.293161	6577.007416	15.156659	-0.058646	4.379928
296.190836	6569.007370	15.161664	-0.058621	4.377356
296.262933	6560.964237	15.166669	-0.058629	4.374770
296.172202	6553.012268	15.171674	-0.058607	4.372210
296.022887	6544.942021	15.176679	-0.058574	4.369611
296.111102	6537.024248	15.181683	-0.058585	4.367061
296.138452	6528.913757	15.186688	-0.058584	4.364446
296.140748	6521.000194	15.191693	-0.058580	4.361894
296.159545	6512.998113	15.196698	-0.058578	4.359311
295.919735	6504.989434	15.201703	-0.058528	4.356723
296.308886	6496.960561	15.206707	-0.058595	4.354131
295.982429	6488.864771	15.211712	-0.058528	4.351512
295.848079	6480.897447	15.216717	-0.058498	4.348933
295.779492	6472.898855	15.221722	-0.058480	4.346344
295.713904	6464.911750	15.226727	-0.058462	4.343756
295.663979	6456.970520	15.231731	-0.058447	4.341182
295.619744	6448.982900	15.236736	-0.058434	4.338591
295.913106	6440.926543	15.241741	-0.058483	4.335979
295.705184	6432.953921	15.246746	-0.058439	4.333389
295.506739	6424.915823	15.251751	-0.058396	4.330776
295.509964	6416.954113	15.256755	-0.058391	4.328188
295.450876	6408.928498	15.261760	-0.058375	4.325577
295.508812	6400.986673	15.266765	-0.058380	4.322993
295.555972	6392.942486	15.271770	-0.058384	4.320373
295.444678	6384.974750	15.276775	-0.058358	4.317776
295.379665	6376.950501	15.281779	-0.058340	4.315159
295.180890	6368.917010	15.286784	-0.058297	4.312537
295.382369	6360.906944	15.291789	-0.058330	4.309924
295.186104	6352.927200	15.296794	-0.058288	4.307315
295.395946	6344.848277	15.301799	-0.058321	4.304676
295.576858	6336.973413	15.306803	-0.058350	4.302102
295.472796	6328.870636	15.311808	-0.058325	4.299450
295.235272	6320.964852	15.316813	-0.058275	4.296859
295.180281	6312.936619	15.321818	-0.058259	4.294228
295.140411	6304.892022	15.326823	-0.058246	4.291590
295.293894	6296.912309	15.331827	-0.058270	4.288974
295.048633	6288.874136	15.336832	-0.058218	4.286333
295.245580	6280.923991	15.341837	-0.058250	4.283724
295.205220	6272.937142	15.346842	-0.058237	4.281098
295.039490	6264.915706	15.351847	-0.058201	4.278459
295.083259	6256.927110	15.356851	-0.058203	4.275831
295.029997	6248.861567	15.361856	-0.058188	4.273174
294.924110	6240.853595	15.366861	-0.058163	4.270535
294.669935	6232.877240	15.371866	-0.058110	4.267903
294.825235	6224.849668	15.376871	-0.058133	4.265256
294.873561	6216.921591	15.381875	-0.058137	4.262640
294.799480	6208.868421	15.386880	-0.058118	4.259979
294.774685	6200.903034	15.391885	-0.058108	4.257346
294.736718	6192.891045	15.396890	-0.058095	4.254697
294.528770	6184.866099	15.401895	-0.058051	4.252039
294.757345	6176.876618	15.406899	-0.058088	4.249396
294.772879	6168.908313	15.411904	-0.058086	4.246756
294.617564	6160.897974	15.416909	-0.058051	4.244099
294.534238	6152.933969	15.421914	-0.058030	4.241456
294.517429	6144.902564	15.426919	-0.058022	4.238790
294.554680	6136.904750	15.431923	-0.058023	4.236133
294.564040	6128.866736	15.436928	-0.058020	4.233462
294.405666	6120.899660	15.441933	-0.057985	4.230811
294.523328	6112.907088	15.446938	-0.058001	4.228152
294.214374	6104.915162	15.451943	-0.057938	4.225488
294.363157	6096.945790	15.456947	-0.057960	4.222834
294.432393	6088.911665	15.461952	-0.057968	4.220156
294.308620	6080.968850	15.466957	-0.057939	4.217504
294.410402	6072.910235	15.471962	-0.057953	4.214815
294.294611	6064.910044	15.476967	-0.057926	4.212141
294.398033	6056.898959	15.481971	-0.057940	4.209465
294.240413	6048.956007	15.486976	-0.057905	4.206806
294.322576	6040.881119	15.491981	-0.057915	4.204104
294.287588	6032.961349	15.496986	-0.057903	4.201452
294.041051	6024.913528	15.501991	-0.057852	4.198752
294.000019	6016.961313	15.506995	-0.057839	4.196085
293.914103	6008.846322	15.512000	-0.057817	4.193361
293.866080	6000.766113	15.517005	-0.057803	4.190647
293.864117	5992.871751	15.522010	-0.057797	4.187995
293.991626	5984.827836	15.527015	-0.057815	4.185292
293.917970	5976.915278	15.532019	-0.057796	4.182629
293.668369	5968.874476	15.537024	-0.057744	4.179920
293.632945	5960.914421	15.542029	-0.057732	4.177238
293.616641	5952.903315	15.547034	-0.057724	4.174537
293.713502	5944.873288	15.552039	-0.057736	4.171830
293.794199	5936.865628	15.557043	-0.057746	4.169128
293.645187	5928.903202	15.562048	-0.057713	4.166437
293.557233	5920.883896	15.567053	-0.057691	4.163726
293.626932	5912.942019	15.572058	-0.057698	4.161041
293.563335	5904.910198	15.577063	-0.057681	4.158322
293.585378	5896.886248	15.582067	-0.057680	4.155606
293.402775	5888.872782	15.587072	-0.057640	4.152888
293.548783	5880.850450	15.592077	-0.057662	4.150170
293.532980	5872.868420	15.597082	-0.057654	4.147462
293.288496	5864.817846	15.602087	-0.057603	4.144726
293.280638	5856.953574	15.607091	-0.057596	4.142054
293.369905	5848.892629	15.612096	-0.057607	4.139314
293.202757	5840.894784	15.617101	-0.057570	4.136592
293.184899	5832.878579	15.622106	-0.057562	4.133863
293.092901	5824.854785	15.627111	-0.057539	4.131129
293.103906	5816.848173	15.632115	-0.057536	4.128400
292.991603	5808.832147	15.637120	-0.057509	4.125664
292.904400	5800.882751	15.642125	-0.057488	4.122950
293.225680	5792.881518	15.647130	-0.057542	4.120221
292.853401	5784.875583	15.652135	-0.057467	4.117480
292.949790	5776.890512	15.657139	-0.057480	4.114751
292.971205	5768.821407	15.662144	-0.057478	4.111990
292.923414	5760.846911	15.667149	-0.057464	4.109258
292.864846	5752.852651	15.672154	-0.057448	4.106518
292.630513	5744.835867	15.677159	-0.057399	4.103766
292.809688	5736.896055	15.682163	-0.057427	4.101044
292.875451	5728.888551	15.687168	-0.057433	4.098295
292.619033	5720.894314	15.692173	-0.057380	4.095545
292.643814	5712.896450	15.697178	-0.057379	4.092796
292.626829	5704.870212	15.702183	-0.057371	4.090034
292.552653	5696.904231	15.707187	-0.057352	4.087290
292.643248	5688.875540	15.712192	-0.057363	4.084526
292.685621	5680.903956	15.717197	-0.057365	4.081778
292.498697	5672.912484	15.722202	-0.057325	4.079018
292.446137	5664.915704	15.727207	-0.057310	4.076257
292.523430	5656.907408	15.732211	-0.057319	4.073491
292.350282	5648.864989	15.737216	-0.057281	4.070709
292.432757	5640.888143	15.742221	-0.057291	4.067950
292.546700	5632.880236	15.747226	-0.057307	4.065180
292.495051	5624.915168	15.752231	-0.057292	4.062420
292.346289	5616.926227	15.757235	-0.057259	4.059649
292.437911	5608.940965	15.762240	-0.057270	4.056880
292.257694	5600.912181	15.767245	-0.057231	4.054091
292.275383	5592.912189	15.772250	-0.057229	4.051312
292.177991	5584.894680	15.777255	-0.057206	4.048524
292.113493	5576.918144	15.782259	-0.057188	4.045748
292.207255	5568.935036	15.787264	-0.057200	4.042971
292.129732	5560.892089	15.792269	-0.057180	4.040168
292.219450	5552.956857	15.797274	-0.057192	4.037404
291.944438	5544.915625	15.802279	-0.057135	4.034595
291.998937	5536.810473	15.807283	-0.057140	4.031767
291.811730	5528.847447	15.812288	-0.057099	4.028983
291.822482	5520.838540	15.817293	-0.057096	4.026183
291.812451	5512.891436	15.822298	-0.057089	4.023404
291.598436	5504.885672	15.827303	-0.057043	4.020598
291.736768	5496.930652	15.832307	-0.057064	4.017814
291.831369	5488.887759	15.837312	-0.057076	4.014996
291.672377	5480.887559	15.842317	-0.057041	4.012188
291.673891	5472.868084	15.847322	-0.057036	4.009373
291.716451	5464.850630	15.852327	-0.057038	4.006558
291.544787	5456.923035	15.857331	-0.057001	4.003768
291.404678	5448.917099	15.862336	-0.056969	4.000950
291.543923	5440.918365	15.867341	-0.056990	3.998137
291.491836	5432.913562	15.872346	-0.056975	3.995316
291.386563	5424.872607	15.877351	-0.056950	3.992480
291.547800	5416.885319	15.882355	-0.056974	3.989666
291.501089	5408.886692	15.887360	-0.056960	3.986841
291.415124	5400.868192	15.892365	-0.056939	3.984008
291.444447	5392.919818	15.897370	-0.056939	3.981198
291.335017	5384.928840	15.902375	-0.056913	3.978370
291.275720	5376.903334	15.907379	-0.056896	3.975528
291.170218	5368.905161	15.912384	-0.056871	3.972693
291.343763	5360.851992	15.917389	-0.056898	3.969841
291.227665	5352.924768	15.922394	-0.056871	3.967027
290.939867	5344.898900	15.927399	-0.056812	3.964173
290.884683	5336.955634	15.932403	-0.056796	3.961350
290.806478	5328.980544	15.937408	-0.056776	3.958513
290.817919	5320.984070	15.942413	-0.056773	3.955668
290.865815	5312.924087	15.947418	-0.056777	3.952799
290.751705	5304.862945	15.952423	-0.056750	3.949925
290.796240	5296.917255	15.957427	-0.056753	3.947093
290.684504	5288.926329	15.962432	-0.056727	3.944240
290.692395	5280.971177	15.967437	-0.056723	3.941399
290.630597	5273.001632	15.972442	-0.056706	3.938551
290.536334	5264.981024	15.977447	-0.056683	3.935681
290.631422	5256.970822	15.982451	-0.056695	3.932816
290.524649	5248.961717	15.987456	-0.056670	3.929946
290.506151	5240.963657	15.992461	-0.056661	3.927079
290.468995	5232.967173	15.997466	-0.056648	3.924211
290.344056	5224.975789	16.002471	-0.056620	3.921341
290.337884	5217.019034	16.007475	-0.056613	3.918483
290.350040	5208.990749	16.012480	-0.056610	3.915597
290.596781	5200.938142	16.017485	-0.056650	3.912705
290.514151	5192.947348	16.022490	-0.056630	3.909828
290.126568	5184.965228	16.027495	-0.056552	3.906945
290.183238	5176.995584	16.032499	-0.056557	3.904073
290.349448	5168.949963	16.037504	-0.056583	3.901174
290.210067	5160.960791	16.042509	-0.056551	3.898287
290.048911	5153.009842	16.047514	-0.056516	3.895411
290.147514	5144.953642	16.052519	-0.056529	3.892500
290.149648	5136.951651	16.057523	-0.056524	3.889605
290.207074	5128.975966	16.062528	-0.056529	3.886718
289.979944	5120.967064	16.067533	-0.056481	3.883811
290.088436	5112.997124	16.072538	-0.056496	3.880923
289.900555	5104.972417	16.077543	-0.056456	3.878007
290.193636	5096.981256	16.082547	-0.056505	3.875111
290.081177	5088.762815	16.087552	-0.056478	3.872121
290.114203	5080.796859	16.092557	-0.056479	3.869224
290.060636	5072.878434	16.097562	-0.056464	3.866341
290.121509	5064.875749	16.102567	-0.056469	3.863427
289.868975	5056.954445	16.107571	-0.056417	3.860534
289.709938	5048.989577	16.112576	-0.056382	3.857625
289.606940	5040.942230	16.117581	-0.056357	3.854685
289.801257	5032.994811	16.122586	-0.056388	3.851785
289.627548	5024.940586	16.127591	-0.056350	3.848836
289.768013	5016.945049	16.132595	-0.056371	3.845913
289.733395	5008.994295	16.137600	-0.056359	3.843000
289.577059	5001.006177	16.142605	-0.056325	3.840069
289.599272	4993.060982	16.147610	-0.056323	3.837155
289.357036	4985.019424	16.152615	-0.056273	3.834199
289.431581	4977.002763	16.157619	-0.056281	3.831255
289.348062	4969.003770	16.162624	-0.056260	3.828313
289.360332	4960.987694	16.167629	-0.056257	3.825364
289.462057	4953.057438	16.172634	-0.056271	3.822446
289.492338	4945.015347	16.177639	-0.056271	3.819483
289.177400	4937.071315	16.182643	-0.056207	3.816547
289.164033	4929.067058	16.187648	-0.056199	3.813592
289.069803	4921.006957	16.192653	-0.056176	3.810613
289.190631	4913.060578	16.197658	-0.056193	3.807679
289.261665	4904.999173	16.202663	-0.056201	3.804698
289.218465	4897.105020	16.207667	-0.056187	3.801775
289.221977	4889.083658	16.212672	-0.056183	3.798803
289.155145	4881.085352	16.217677	-0.056165	3.795836
289.200833	4873.057243	16.222682	-0.056168	3.792858
288.927042	4865.034224	16.227687	-0.056111	3.789872
288.932725	4857.028718	16.232691	-0.056107	3.786897
288.984862	4849.067004	16.237696	-0.056111	3.783937
288.919807	4841.039725	16.242701	-0.056094	3.780947
288.738858	4833.107894	16.247706	-0.056055	3.777988
288.724240	4825.049285	16.252711	-0.056046	3.774983
288.784692	4817.099615	16.257715	-0.056052	3.772018
288.692948	4809.070148	16.262720	-0.056030	3.769017
288.644745	4801.048646	16.267725	-0.056015	3.766018
288.804476	4793.095113	16.272730	-0.056040	3.763047
288.583667	4785.061911	16.277735	-0.055993	3.760035
288.580455	4777.142659	16.282739	-0.055987	3.757068
288.664569	4769.094433	16.287744	-0.055997	3.754053
288.479702	4761.061804	16.292749	-0.055957	3.751034
288.485973	4753.097825	16.297754	-0.055953	3.748044
288.560868	4745.048744	16.302759	-0.055962	3.745021
288.496166	4737.137653	16.307763	-0.055944	3.742043
288.367637	4729.101758	16.312768	-0.055915	3.739015
288.246108	4721.131638	16.317773	-0.055887	3.736010
288.449843	4713.143349	16.322778	-0.055919	3.733003
288.111509	4705.087352	16.327783	-0.055851	3.729955
288.137771	4697.123220	16.332787	-0.055850	3.726948
288.084394	4689.127643	16.337792	-0.055835	3.723924
288.177125	4681.154841	16.342797	-0.055847	3.720911
288.308467	4673.183520	16.347802	-0.055866	3.717896
288.065194	4665.168534	16.352807	-0.055815	3.714853
288.084185	4657.051167	16.357811	-0.055813	3.711776
287.992682	4649.065257	16.362816	-0.055791	3.708743
287.807593	4641.081307	16.367821	-0.055751	3.705705
287.911371	4633.170600	16.372826	-0.055765	3.702701
287.754149	4625.151220	16.377831	-0.055730	3.699646
287.640730	4617.199604	16.382835	-0.055703	3.696615
287.890771	4609.177509	16.387840	-0.055745	3.693565
287.912031	4601.145069	16.392845	-0.055743	3.690502
287.861664	4593.180431	16.397850	-0.055728	3.687460
287.490190	4585.176644	16.402855	-0.055654	3.684393
287.569639	4577.248544	16.407859	-0.055663	3.681364
287.454760	4569.219985	16.412864	-0.055636	3.678289
287.362902	4561.193404	16.417869	-0.055614	3.675212
287.507569	4553.209870	16.422874	-0.055635	3.672156
287.460213	4545.170971	16.427879	-0.055621	3.669071
287.343375	4537.200433	16.432883	-0.055594	3.666007
287.270875	4529.234435	16.437888	-0.055575	3.662944
287.277779	4521.217021	16.442893	-0.055571	3.659861
287.307155	4513.276187	16.447898	-0.055571	3.656805
287.154080	4505.194822	16.452903	-0.055537	3.653688
287.522680	4497.184369	16.457907	-0.055600	3.650609
287.430310	4489.221778	16.462912	-0.055577	3.647534
287.232760	4481.197218	16.467917	-0.055535	3.644429
287.207249	4473.294495	16.472922	-0.055525	3.641374
287.051487	4465.269480	16.477927	-0.055490	3.638265
287.099566	4457.269526	16.482931	-0.055494	3.635168
286.961994	4449.220010	16.487936	-0.055463	3.632045
286.890687	4441.182528	16.492941	-0.055444	3.628926
287.123358	4433.205533	16.497946	-0.055482	3.625835
286.971792	4425.224392	16.502951	-0.055448	3.622730
287.015671	4417.249287	16.507955	-0.055451	3.619630
287.165431	4409.315242	16.512960	-0.055474	3.616546
286.768596	4401.274273	16.517965	-0.055394	3.613403
286.940527	4393.270666	16.522970	-0.055421	3.610287
286.913654	4385.270413	16.527975	-0.055410	3.607164
286.845291	4377.260083	16.532979	-0.055392	3.604034
286.761312	4369.317739	16.537984	-0.055371	3.600927
286.756117	4361.366287	16.542989	-0.055365	3.597816
286.642090	4353.371352	16.547994	-0.055338	3.594682
286.371479	4345.330216	16.552999	-0.055282	3.591523
286.564697	4337.315332	16.558003	-0.055313	3.588384
286.587135	4329.350730	16.563008	-0.055312	3.585258
286.269750	4321.357359	16.568013	-0.055247	3.582108
286.273896	4313.416820	16.573018	-0.055242	3.578985
286.282921	4305.362362	16.578023	-0.055239	3.575815
286.390420	4297.346662	16.583027	-0.055253	3.572659
286.349295	4289.368677	16.588032	-0.055240	3.569512
286.414518	4281.373334	16.593037	-0.055247	3.566358
286.293759	4273.415332	16.598042	-0.055219	3.563211
286.195508	4265.396463	16.603047	-0.055195	3.560037
286.147994	4257.425194	16.608051	-0.055181	3.556881
286.156994	4249.370171	16.613056	-0.055177	3.553691
286.124941	4241.300251	16.618061	-0.055166	3.550491
286.252652	4233.333441	16.623066	-0.055184	3.547333
286.164551	4225.341110	16.628071	-0.055162	3.544156
285.988063	4217.422284	16.633075	-0.055124	3.541003
285.999635	4209.425863	16.638080	-0.055121	3.537822
285.995436	4201.399428	16.643085	-0.055115	3.534625
286.126032	4193.409215	16.648090	-0.055133	3.531444
285.930864	4185.407822	16.653095	-0.055092	3.528246
285.913283	4177.394813	16.658099	-0.055083	3.525045
286.011216	4169.470080	16.663104	-0.055096	3.521881
285.885188	4161.430689	16.668109	-0.055067	3.518661
285.624324	4153.501788	16.673114	-0.055013	3.515478
285.629667	4145.443739	16.678119	-0.055008	3.512249
285.710686	4137.448736	16.683123	-0.055018	3.509044
285.710343	4129.450962	16.688128	-0.055013	3.505833
285.717939	4121.467672	16.693133	-0.055009	3.502624
285.701292	4113.487373	16.698138	-0.055000	3.499414
285.413658	4105.526952	16.703143	-0.054941	3.496200
285.439287	4097.526345	16.708147	-0.054940	3.492976
285.438440	4089.500374	16.713152	-0.054935	3.489739
285.408790	4081.515028	16.718157	-0.054924	3.486514
285.451300	4073.571579	16.723162	-0.054926	3.483305
285.218925	4065.564493	16.728167	-0.054878	3.480059
285.379021	4057.596458	16.733171	-0.054902	3.476838
285.185465	4049.583625	16.738176	-0.054861	3.473584
285.202788	4041.516286	16.743181	-0.054858	3.470312
285.242350	4033.539329	16.748186	-0.054860	3.467075
284.867036	4025.569847	16.753191	-0.054785	3.463824
285.169705	4017.563851	16.758195	-0.054836	3.460577
285.205923	4009.591931	16.763200	-0.054837	3.457332
285.094515	4001.589561	16.768205	-0.054811	3.454067
284.847297	3993.616449	16.773210	-0.054760	3.450807
284.939617	3985.611385	16.778215	-0.054771	3.447541
285.017588	3977.581435	16.783219	-0.054780	3.444262
284.966691	3969.633617	16.788224	-0.054766	3.441009
284.800351	3961.659282	16.793229	-0.054729	3.437738
284.958058	3953.640353	16.798234	-0.054753	3.434456
284.870446	3945.620898	16.803239	-0.054731	3.431163
284.844488	3937.628460	16.808243	-0.054721	3.427880
284.683670	3929.633499	16.813248	-0.054686	3.424588
284.705714	3921.669197	16.818253	-0.054684	3.421312
284.719760	3913.707116	16.823258	-0.054682	3.418033
284.538093	3905.718118	16.828263	-0.054642	3.414734
284.474083	3897.721901	16.833267	-0.054625	3.411432
284.309402	3889.707816	16.838272	-0.054589	3.408116
284.335030	3881.715223	16.843277	-0.054588	3.404812
284.375197	3873.752544	16.848282	-0.054590	3.401518
284.279844	3865.744103	16.853287	-0.054567	3.398197
284.283657	3857.771359	16.858291	-0.054562	3.394891
284.502765	3849.642468	16.863296	-0.054598	3.391525
284.458315	3841.671398	16.868301	-0.054584	3.388211
284.315276	3833.723968	16.873306	-0.054552	3.384901
284.249031	3825.774896	16.878311	-0.054534	3.381590
284.318147	3817.760027	16.883315	-0.054542	3.378252
283.970700	3809.792903	16.888320	-0.054471	3.374917
284.050407	3801.760859	16.893325	-0.054481	3.371566
284.152298	3793.798339	16.898330	-0.054494	3.368242
283.943679	3785.777687	16.903335	-0.054450	3.364879
283.920029	3777.844688	16.908339	-0.054440	3.361556
283.939587	3769.857034	16.913344	-0.054439	3.358208
283.767782	3761.849932	16.918349	-0.054401	3.354842
283.973964	3753.828755	16.923354	-0.054434	3.351480
283.945164	3745.802447	16.928359	-0.054423	3.348104
283.830771	3737.829480	16.933363	-0.054397	3.344744
283.888032	3729.900785	16.938368	-0.054402	3.341406
283.840871	3721.888449	16.943373	-0.054388	3.338025
283.930066	3713.900455	16.948378	-0.054399	3.334656
283.617822	3705.905371	16.953383	-0.054335	3.331266
283.532585	3697.895743	16.958387	-0.054314	3.327874
283.426605	3689.914570	16.963392	-0.054289	3.324491
283.561782	3681.940236	16.968397	-0.054308	3.321116
283.531646	3673.966463	16.973402	-0.054297	3.317731
283.346058	3665.967566	16.978407	-0.054257	3.314326
283.517138	3657.915305	16.983411	-0.054284	3.310909
283.220008	3649.950960	16.988416	-0.054223	3.307508
283.059766	3641.971059	16.993421	-0.054188	3.304102
283.294179	3634.005258	16.998426	-0.054226	3.300713
283.244521	3626.010054	17.003431	-0.054211	3.297298
283.267480	3618.023962	17.008435	-0.054210	3.293885
283.218409	3610.018323	17.013440	-0.054196	3.290458
283.244622	3602.015740	17.018445	-0.054195	3.287032
283.105258	3594.058976	17.023450	-0.054164	3.283615
282.952838	3586.074664	17.028455	-0.054130	3.280183
282.998796	3578.112066	17.033459	-0.054133	3.276763
283.009616	3570.083317	17.038464	-0.054130	3.273311
282.978790	3562.029860	17.043469	-0.054118	3.269842
283.118851	3554.059903	17.048474	-0.054139	3.266413
283.110747	3546.093696	17.053479	-0.054132	3.262975
282.943003	3538.116535	17.058483	-0.054096	3.259523
282.893320	3530.158741	17.063488	-0.054081	3.256081
282.702328	3522.124323	17.068493	-0.054040	3.252596
283.023803	3514.119862	17.073498	-0.054094	3.249140
282.706686	3506.154606	17.078503	-0.054030	3.245673
282.794190	3498.170685	17.083507	-0.054041	3.242209
282.673009	3490.205969	17.088512	-0.054013	3.238742
282.442097	3482.229913	17.093517	-0.053964	3.235262
282.382628	3474.193603	17.098522	-0.053948	3.231759
282.517782	3466.143609	17.103527	-0.053967	3.228254
282.371843	3458.149276	17.108531	-0.053935	3.224758
282.592289	3450.214362	17.113536	-0.053971	3.221299
282.452708	3442.214649	17.118541	-0.053939	3.217794
282.245065	3434.252207	17.123546	-0.053895	3.214297
282.322617	3426.229692	17.128551	-0.053904	3.210783
282.251972	3418.257633	17.133555	-0.053885	3.207281
282.181409	3410.277272	17.138560	-0.053867	3.203771
282.190089	3402.284000	17.143565	-0.053863	3.200255
282.336203	3394.350941	17.148570	-0.053885	3.196767
282.296697	3386.299748	17.153575	-0.053872	3.193216
281.947965	3378.310341	17.158579	-0.053802	3.189675
281.909899	3370.356802	17.163584	-0.053789	3.186159
281.904160	3362.351129	17.168589	-0.053783	3.182618
282.274664	3354.328156	17.173594	-0.053846	3.179080
281.984588	3346.399230	17.178599	-0.053787	3.175553
281.946478	3338.360794	17.183603	-0.053774	3.171983
281.775372	3330.401142	17.188608	-0.053737	3.168439
281.743037	3322.389370	17.193613	-0.053726	3.164874
281.841167	3314.460889	17.198618	-0.053738	3.161347
281.816536	3306.441146	17.203623	-0.053728	3.157771
281.703898	3298.460736	17.208627	-0.053702	3.154204
281.826081	3290.426727	17.213632	-0.053719	3.150619
281.469784	3282.472936	17.218637	-0.053648	3.147045
281.466309	3274.479212	17.223642	-0.053641	3.143465
281.386614	3266.510423	17.228647	-0.053621	3.139889
281.549711	3258.523434	17.233651	-0.053646	3.136310
281.337071	3250.528998	17.238656	-0.053601	3.132708
281.329453	3242.513941	17.243661	-0.053594	3.129102
281.365320	3234.544706	17.248666	-0.053596	3.125514
281.268352	3226.585994	17.253671	-0.053572	3.121920
281.299414	3218.605140	17.258675	-0.053572	3.118318
281.117525	3210.642231	17.263680	-0.053533	3.114711
281.169199	3202.595746	17.268685	-0.053537	3.111072
281.379948	3194.594436	17.273690	-0.053571	3.107456
281.194697	3186.619218	17.278695	-0.053531	3.103830
281.142894	3178.660663	17.283699	-0.053516	3.100214
281.251024	3170.681650	17.288704	-0.053531	3.096591
281.183429	3162.676809	17.293709	-0.053513	3.092944
280.890100	3154.704184	17.298714	-0.053453	3.089297
280.976083	3146.705578	17.303719	-0.053463	3.085652
280.765706	3138.745669	17.308723	-0.053419	3.082006
280.739200	3130.782800	17.313728	-0.053408	3.078363
280.814170	3122.742074	17.318733	-0.053417	3.074685
280.850131	3114.663856	17.323738	-0.053418	3.070983
280.706829	3106.716955	17.328743	-0.053386	3.067329
280.606719	3098.742601	17.333747	-0.053362	3.063659
280.662921	3090.772039	17.338752	-0.053367	3.059995
280.615741	3082.802627	17.343757	-0.053353	3.056321
280.619856	3074.818615	17.348762	-0.053348	3.052639
280.658600	3066.821079	17.353767	-0.053350	3.048948
280.598156	3058.838708	17.358771	-0.053333	3.045255
280.524568	3050.891677	17.363776	-0.053314	3.041573
280.413828	3042.930550	17.368781	-0.053288	3.037878
280.420628	3034.935384	17.373786	-0.053284	3.034168
280.581293	3026.887008	17.378791	-0.053308	3.030437
280.448867	3018.923893	17.383795	-0.053278	3.026726
280.496241	3010.938477	17.388800	-0.053282	3.023010
280.243719	3002.976103	17.393805	-0.053229	3.019284
280.146220	2995.034206	17.398810	-0.053206	3.015572
280.103978	2987.008914	17.403815	-0.053192	3.011818
280.123596	2978.996490	17.408819	-0.053191	3.008069
280.039086	2971.048941	17.413824	-0.053170	3.004340
280.040658	2963.057682	17.418829	-0.053164	3.000591
280.071617	2955.113823	17.423834	-0.053165	2.996860
280.121088	2947.090328	17.428839	-0.053169	2.993089
279.961153	2939.075260	17.433843	-0.053133	2.989306
279.876926	2931.121272	17.438848	-0.053112	2.985551
279.870274	2923.144639	17.443853	-0.053106	2.981784
280.011290	2915.156422	17.448858	-0.053126	2.978014
279.967244	2907.159767	17.453863	-0.053113	2.974227
279.904792	2899.152252	17.458867	-0.053096	2.970428
279.990694	2891.206842	17.463872	-0.053106	2.966662
279.576286	2883.239145	17.468877	-0.053024	2.962855
279.580783	2875.272947	17.473882	-0.053019	2.959064
279.559401	2867.298130	17.478887	-0.053010	2.955264
279.458023	2859.266998	17.483891	-0.052985	2.951428
279.635731	2851.282177	17.488896	-0.053013	2.947623
279.493025	2843.307034	17.493901	-0.052981	2.943801
279.494333	2835.339084	17.498906	-0.052976	2.939986
279.508607	2827.371613	17.503911	-0.052973	2.936166
279.245171	2819.361553	17.508915	-0.052919	2.932306
279.445625	2811.367412	17.513920	-0.052951	2.928473
279.252694	2803.385769	17.518925	-0.052909	2.924621
279.367194	2795.443245	17.523930	-0.052925	2.920798
279.411542	2787.461219	17.528935	-0.052928	2.916948
279.296244	2779.440104	17.533939	-0.052901	2.913065
279.225853	2771.402887	17.538944	-0.052882	2.909171
279.106526	2763.432722	17.543949	-0.052855	2.905303
278.925689	2755.513461	17.548954	-0.052816	2.901450
278.734236	2747.543707	17.553959	-0.052775	2.897567
278.970728	2739.530283	17.558963	-0.052813	2.893681
278.959379	2731.533226	17.563968	-0.052806	2.889784
278.692848	2723.568934	17.568973	-0.052751	2.885884
278.919104	2715.598361	17.573978	-0.052787	2.882002
278.857776	2707.629027	17.578983	-0.052771	2.878101
278.641253	2699.666220	17.583987	-0.052725	2.874188
278.740022	2691.652370	17.588992	-0.052738	2.870262
278.640943	2683.667803	17.593997	-0.052714	2.866335
278.598752	2675.710045	17.599002	-0.052701	2.862418
278.437418	2667.727832	17.604007	-0.052665	2.858478
278.441629	2659.753872	17.609011	-0.052661	2.854545
278.430813	2651.761644	17.614016	-0.052653	2.850597
278.433467	2643.783387	17.619021	-0.052648	2.846651
278.618378	2635.806255	17.624026	-0.052677	2.842710
278.476159	2627.849525	17.629031	-0.052645	2.838756
278.301192	2619.885068	17.634035	-0.052607	2.834791
278.414987	2611.866983	17.639040	-0.052623	2.830809
278.410753	2603.865435	17.644045	-0.052617	2.826824
278.167582	2595.926240	17.649050	-0.052566	2.822850
278.256244	2587.926030	17.654055	-0.052577	2.818859
278.235915	2579.957079	17.659059	-0.052568	2.814872
278.139248	2571.972070	17.664064	-0.052545	2.810867
277.745411	2564.017746	17.669069	-0.052466	2.806854
278.013494	2556.027948	17.674074	-0.052510	2.802856
278.013562	2548.062345	17.679079	-0.052505	2.798849
277.925749	2540.092917	17.684083	-0.052483	2.794829
277.920718	2532.087078	17.689088	-0.052477	2.790790
277.871218	2524.091815	17.694093	-0.052462	2.786747
277.886762	2516.135770	17.699098	-0.052460	2.782723
277.776911	2508.167643	17.704103	-0.052434	2.778679
277.779223	2500.189496	17.709107	-0.052429	2.774631
277.714174	2492.213052	17.714112	-0.052411	2.770573
277.515672	2484.236349	17.719117	-0.052369	2.766502
277.698193	2476.268491	17.724122	-0.052397	2.762452
277.622127	2468.303438	17.729127	-0.052378	2.758381
277.528868	2460.325351	17.734131	-0.052355	2.754298
277.285626	2452.286614	17.739136	-0.052304	2.750167
277.256856	2444.296865	17.744141	-0.052294	2.746069
277.348931	2436.331520	17.749146	-0.052305	2.741985
277.295764	2428.388499	17.754151	-0.052290	2.737897
277.339819	2420.393150	17.759155	-0.052293	2.733782
277.148507	2412.435328	17.764160	-0.052252	2.729665
277.102046	2404.469983	17.769165	-0.052238	2.725548
277.044645	2396.524032	17.774170	-0.052222	2.721433
277.086490	2388.538556	17.779175	-0.052224	2.717298
277.077700	2380.536392	17.784179	-0.052217	2.713145
276.926588	2372.575516	17.789184	-0.052183	2.708998
276.884694	2364.585060	17.794189	-0.052170	2.704836
276.970945	2356.629841	17.799194	-0.052181	2.700694
277.063974	2348.661464	17.804199	-0.052193	2.696539
276.871760	2340.677022	17.809203	-0.052151	2.692352
276.887545	2332.689556	17.814208	-0.052149	2.688169
276.615951	2324.749818	17.819213	-0.052093	2.683987
276.661047	2316.771231	17.824218	-0.052096	2.679798
276.788784	2308.819384	17.829223	-0.052114	2.675621
276.490450	2300.817354	17.834227	-0.052053	2.671385
276.548735	2292.835658	17.839232	-0.052059	2.667175
276.693153	2284.825949	17.844237	-0.052080	2.662950
276.619658	2276.889609	17.849242	-0.052061	2.658742
276.493530	2268.931131	17.854247	-0.052032	2.654513
276.574566	2260.923951	17.859251	-0.052042	2.650264
276.474376	2252.979906	17.864256	-0.052018	2.646031
276.392188	2245.019790	17.869261	-0.051997	2.641783
276.229288	2237.080982	17.874266	-0.051961	2.637534
276.266321	2229.078227	17.879271	-0.051963	2.633258
276.328319	2221.068478	17.884275	-0.051969	2.628972
276.098303	2213.143286	17.889280	-0.051921	2.624706
276.132868	2205.157165	17.894285	-0.051922	2.620417
276.333906	2197.183181	17.899290	-0.051954	2.616139
276.166398	2189.220971	17.904295	-0.051917	2.611835
276.185538	2181.233187	17.909299	-0.051915	2.607524
276.123151	2173.282013	17.914304	-0.051898	2.603219
275.890241	2165.330443	17.919309	-0.051850	2.598895
275.772898	2157.384423	17.924314	-0.051822	2.594576
275.727763	2149.197344	17.929319	-0.051808	2.590122
275.771478	2141.246692	17.934323	-0.051811	2.585796
275.815248	2133.325038	17.939328	-0.051814	2.581478
275.815896	2125.373490	17.944333	-0.051809	2.577134
275.751849	2117.424959	17.949338	-0.051791	2.572780
275.741918	2109.434447	17.954343	-0.051784	2.568399
275.622113	2101.488478	17.959347	-0.051756	2.564028
275.640320	2093.557399	17.964352	-0.051754	2.559666
275.581715	2085.611048	17.969357	-0.051738	2.555284
275.438250	2077.635994	17.974362	-0.051706	2.550872
275.465384	2069.661904	17.979367	-0.051705	2.546465
275.472964	2061.690849	17.984371	-0.051701	2.542051
275.312764	2053.758932	17.989376	-0.051666	2.537638
275.427220	2045.746664	17.994381	-0.051682	2.533193
275.486649	2037.767458	17.999386	-0.051688	2.528755
275.284312	2029.838503	18.004391	-0.051645	2.524318
275.121197	2021.893459	18.009395	-0.051609	2.519867
275.280986	2013.938391	18.014400	-0.051633	2.515426
275.175949	2005.911975	18.019405	-0.051608	2.510918
275.117560	1997.956500	18.024410	-0.051592	2.506445
275.118054	1989.981339	18.029415	-0.051587	2.501957
274.867909	1982.058643	18.034419	-0.051535	2.497472
274.905737	1974.090731	18.039424	-0.051536	2.492975
274.926959	1966.077021	18.044429	-0.051535	2.488442
275.043325	1958.117835	18.049434	-0.051551	2.483940
274.733549	1950.203618	18.054439	-0.051488	2.479423
274.651596	1942.266433	18.059443	-0.051467	2.474901
274.899307	1934.236284	18.064448	-0.051508	2.470343
274.799594	1926.268294	18.069453	-0.051484	2.465786
274.683783	1918.341184	18.074458	-0.051457	2.461243
274.629019	1910.390313	18.079463	-0.051441	2.456682
274.460406	1902.429220	18.084467	-0.051405	2.452098
274.382315	1894.466358	18.089472	-0.051385	2.447512
274.444442	1886.487322	18.094477	-0.051391	2.442918
274.659154	1878.521539	18.099482	-0.051425	2.438334
274.542759	1870.566504	18.104487	-0.051398	2.433724
274.423640	1862.544367	18.109491	-0.051371	2.429065
274.231205	1854.622842	18.114496	-0.051330	2.424450
274.202349	1846.665112	18.119501	-0.051319	2.419818
274.176666	1838.721408	18.124506	-0.051309	2.415185
274.143087	1830.735795	18.129511	-0.051297	2.410518
274.193613	1822.755279	18.134515	-0.051301	2.405852
274.188763	1814.832686	18.139520	-0.051295	2.401206
274.011554	1806.902474	18.144525	-0.051256	2.396533
273.954468	1798.926228	18.149530	-0.051240	2.391834
273.905125	1790.960950	18.154535	-0.051226	2.387132
273.728932	1783.002512	18.159539	-0.051187	2.382415
273.846826	1775.056064	18.164544	-0.051204	2.377719
273.902319	1767.078410	18.169549	-0.051209	2.372990
273.884889	1759.112253	18.174554	-0.051200	2.368253
273.767768	1751.185148	18.179559	-0.051173	2.363522
273.817414	1743.231378	18.184563	-0.051177	2.358778
273.780726	1735.295837	18.189568	-0.051165	2.354029
273.449849	1727.317488	18.194573	-0.051098	2.349221
273.588722	1719.335172	18.199578	-0.051118	2.344439
273.571995	1711.392476	18.204583	-0.051109	2.339658
273.388162	1703.468798	18.209587	-0.051070	2.334865
273.436682	1695.484994	18.214592	-0.051073	2.330045
273.411910	1687.520439	18.219597	-0.051063	2.325221
273.580364	1679.559687	18.224602	-0.051089	2.320404
273.408880	1671.663052	18.229607	-0.051052	2.315589
273.243883	1663.672004	18.234611	-0.051016	2.310707
273.327582	1655.719815	18.239616	-0.051026	2.305858
272.911134	1647.803440	18.244621	-0.050943	2.300980
273.022115	1639.840838	18.249626	-0.050958	2.296107
272.981715	1631.880345	18.254631	-0.050945	2.291212
273.001219	1623.893429	18.259635	-0.050944	2.286295
273.151935	1615.948023	18.264640	-0.050966	2.281405
273.279968	1607.993927	18.269645	-0.050985	2.276497
272.917804	1600.032347	18.274650	-0.050912	2.271531
272.671932	1592.078833	18.279655	-0.050861	2.266570
272.711074	1584.124902	18.284659	-0.050863	2.261622
272.868508	1576.183907	18.289664	-0.050887	2.256682
272.541661	1568.259198	18.294669	-0.050820	2.251699
272.376252	1560.318315	18.299674	-0.050784	2.246708
272.442044	1552.370134	18.304679	-0.050791	2.241722
272.320840	1544.434228	18.309683	-0.050763	2.236717
272.207877	1536.494491	18.314688	-0.050737	2.231698
272.182996	1528.508800	18.319693	-0.050727	2.226647
272.200820	1520.567479	18.324698	-0.050724	2.221616
272.124165	1512.643392	18.329703	-0.050705	2.216576
272.230857	1504.648881	18.334707	-0.050719	2.211497
272.434744	1496.691953	18.339712	-0.050752	2.206438
272.000180	1488.801931	18.344717	-0.050665	2.201353
271.990722	1480.870653	18.349722	-0.050658	2.196268
272.230267	1472.868412	18.354727	-0.050698	2.191149
272.168107	1464.904885	18.359731	-0.050681	2.186015
272.205719	1456.983631	18.364736	-0.050682	2.180905
272.143259	1449.045946	18.369741	-0.050665	2.175763
271.971454	1441.113508	18.374746	-0.050628	2.170603
271.725858	1433.201191	18.379751	-0.050577	2.165436
271.669021	1425.266181	18.384755	-0.050561	2.160260
272.026471	1417.305166	18.389760	-0.050622	2.155093
271.630933	1409.357721	18.394765	-0.050543	2.149852
271.518276	1401.442651	18.399770	-0.050516	2.144646
271.627081	1393.495461	18.404775	-0.050531	2.139427
271.521256	1385.552274	18.409779	-0.050506	2.134177
271.287333	1377.635542	18.414784	-0.050457	2.128920
271.313263	1369.676202	18.419789	-0.050457	2.123646
271.525561	1361.741417	18.424794	-0.050491	2.118394
271.279970	1353.805135	18.429799	-0.050440	2.113083
271.109580	1345.827682	18.434803	-0.050402	2.107739
271.180708	1337.889190	18.439808	-0.050410	2.102430
271.076213	1329.962667	18.444813	-0.050385	2.097099
271.139831	1322.014139	18.449818	-0.050392	2.091756
271.387150	1314.058712	18.454823	-0.050433	2.086413
271.175638	1306.161138	18.459827	-0.050388	2.081050
270.894325	1298.296064	18.464832	-0.050330	2.075688
270.899063	1290.305934	18.469837	-0.050326	2.070256
271.016811	1282.356155	18.474842	-0.050342	2.064848
270.881884	1274.464028	18.479847	-0.050312	2.059440
270.631479	1266.548196	18.484851	-0.050260	2.053990
270.867499	1258.579984	18.489856	-0.050298	2.048538
270.809315	1250.655590	18.494861	-0.050282	2.043072
270.665612	1242.770632	18.499866	-0.050250	2.037611
270.544570	1234.833804	18.504871	-0.050222	2.032100
270.626656	1226.855654	18.509875	-0.050232	2.026567
270.577944	1218.949836	18.514880	-0.050217	2.021056
270.494280	1211.029689	18.519885	-0.050196	2.015516
270.588660	1203.072304	18.524890	-0.050208	2.009953
270.518637	1195.169631	18.529895	-0.050190	2.004396
270.509199	1187.247823	18.534899	-0.050183	1.998816
270.468140	1179.348397	18.539904	-0.050170	1.993234
270.340279	1171.413355	18.544909	-0.050141	1.987601
270.309931	1163.477588	18.549914	-0.050130	1.981962
270.308296	1155.572162	18.554919	-0.050124	1.976331
270.282757	1147.632136	18.559923	-0.050114	1.970657
270.212347	1139.735167	18.564928	-0.050095	1.964993
270.149940	1131.834630	18.569933	-0.050078	1.959311
270.206228	1123.899660	18.574938	-0.050083	1.953600
269.976171	1115.963686	18.579943	-0.050035	1.947840
269.872066	1108.052858	18.584947	-0.050010	1.942096
270.067968	1100.116943	18.589952	-0.050042	1.936348
270.033759	1092.191584	18.594957	-0.050030	1.930567
269.808307	1084.294500	18.599962	-0.049982	1.924767
269.844354	1076.408887	18.604967	-0.049984	1.918987
269.974974	1068.434367	18.609971	-0.050003	1.913135
269.923250	1060.542963	18.614976	-0.049988	1.907306
269.789996	1052.644462	18.619981	-0.049958	1.901445
269.738417	1044.741419	18.624986	-0.049943	1.895571
269.574090	1036.843600	18.629991	-0.049907	1.889670
269.319329	1028.959697	18.634995	-0.049854	1.883751
269.360937	1021.072050	18.640000	-0.049856	1.877844
269.330398	1013.131016	18.645005	-0.049845	1.871870
269.213846	1005.213374	18.650010	-0.049818	1.865884
269.084950	997.327209	18.655015	-0.049789	1.859902
269.250505	989.393912	18.660019	-0.049814	1.853898
269.279599	981.473893	18.665024	-0.049814	1.847870
269.125848	973.600575	18.670029	-0.049780	1.841836
269.080516	965.709461	18.675034	-0.049766	1.835781
269.096037	957.789837	18.680039	-0.049764	1.829691
268.950654	949.891018	18.685043	-0.049731	1.823578
268.959436	942.010699	18.690048	-0.049728	1.817477
268.994704	934.085507	18.695053	-0.049729	1.811324
268.846133	926.206995	18.700058	-0.049696	1.805164
268.880360	918.339526	18.705063	-0.049697	1.799014
268.658856	910.437467	18.710067	-0.049650	1.792784
268.518230	902.519425	18.715072	-0.049619	1.786530
268.475138	894.624688	18.720077	-0.049605	1.780285
268.470287	886.739522	18.725082	-0.049599	1.774029
268.498962	878.834232	18.730087	-0.049599	1.767740
268.285728	870.972098	18.735091	-0.049554	1.761432
268.307407	863.104520	18.740096	-0.049553	1.755127
268.226376	855.203353	18.745101	-0.049532	1.748759
268.189932	847.317648	18.750106	-0.049520	1.742386
267.975863	839.477080	18.755111	-0.049475	1.736004
267.901485	831.575977	18.760115	-0.049456	1.729566
268.155966	823.662579	18.765120	-0.049498	1.723137
267.991905	815.808313	18.770125	-0.049462	1.716678
267.859521	807.923239	18.775130	-0.049432	1.710173
267.915930	800.035837	18.780135	-0.049437	1.703666
267.771001	792.179417	18.785139	-0.049405	1.697134
267.761253	784.301271	18.790144	-0.049397	1.690575
267.608132	776.442767	18.795149	-0.049363	1.683989
267.545970	768.584534	18.800154	-0.049347	1.677389
267.692866	760.682636	18.805159	-0.049369	1.670755
267.437871	752.835748	18.810163	-0.049316	1.664086
267.640018	744.956831	18.815168	-0.049348	1.657425
267.421144	737.104315	18.820173	-0.049302	1.650703
267.363395	729.250082	18.825178	-0.049286	1.643973
267.450093	721.391725	18.830183	-0.049297	1.637232
267.077332	713.531009	18.835187	-0.049222	1.630398
267.211659	705.635064	18.840192	-0.049242	1.623575
267.115439	697.791833	18.845197	-0.049218	1.616737
267.045815	689.939765	18.850202	-0.049200	1.609865
267.114159	682.077961	18.855207	-0.049207	1.602975
266.873324	674.264856	18.860211	-0.049157	1.596055
267.049000	666.373952	18.865216	-0.049185	1.589094
266.818215	658.556370	18.870221	-0.049136	1.582110
266.815650	650.714184	18.875226	-0.049130	1.575106
266.693112	642.890235	18.880231	-0.049102	1.568070
266.524956	635.060612	18.885235	-0.049066	1.560990
266.770949	627.192030	18.890240	-0.049106	1.553903
266.723130	619.330376	18.895245	-0.049092	1.546747
266.401014	611.551102	18.900250	-0.049027	1.539592
266.386099	603.719530	18.905255	-0.049019	1.532402
266.255641	595.882977	18.910259	-0.048989	1.525155
266.301421	588.075550	18.915264	-0.048992	1.517928
266.133703	580.248298	18.920269	-0.048956	1.510615
266.124680	572.417516	18.925274	-0.048949	1.503287
266.224132	564.590222	18.930279	-0.048962	1.495944
265.966054	556.793196	18.935283	-0.048908	1.488537
266.069745	548.974813	18.940288	-0.048922	1.481129
265.964769	541.163440	18.945293	-0.048898	1.473659
266.069279	533.283144	18.950298	-0.048912	1.466117
266.031852	525.506212	18.955303	-0.048899	1.458613
265.834731	517.718710	18.960307	-0.048857	1.451034
265.652078	509.951746	18.965312	-0.048818	1.443439
265.500638	502.174061	18.970317	-0.048785	1.435797
265.603370	494.345474	18.975322	-0.048798	1.428106
265.698461	486.544039	18.980327	-0.048811	1.420398
265.164222	478.838132	18.985331	-0.048706	1.412641
265.366019	471.006732	18.990336	-0.048738	1.404836
265.354107	463.230388	18.995341	-0.048731	1.397008
265.224472	455.450621	19.000346	-0.048701	1.389112
265.177192	447.674379	19.005351	-0.048687	1.381189
265.071591	439.914080	19.010355	-0.048662	1.373226
265.136406	432.125075	19.015360	-0.048669	1.365217
264.862486	424.415794	19.020365	-0.048613	1.357184
264.950921	416.614834	19.025370	-0.048624	1.349071
265.126583	408.832749	19.030375	-0.048651	1.340944
264.824383	401.126854	19.035379	-0.048590	1.332763
264.799062	393.379136	19.040384	-0.048580	1.324537
264.684181	385.657798	19.045389	-0.048553	1.316271
264.620220	377.797083	19.050394	-0.048536	1.307812
264.492064	370.081380	19.055399	-0.048507	1.299444
264.434022	362.355796	19.060403	-0.048491	1.291023
264.387908	354.650694	19.065408	-0.048477	1.282572
264.174836	346.966801	19.070413	-0.048432	1.274057
264.284993	339.217378	19.075418	-0.048447	1.265473
264.276483	331.524450	19.080423	-0.048441	1.256870
264.137330	323.829142	19.085427	-0.048409	1.248181
264.039712	316.160928	19.090432	-0.048386	1.239470
263.960745	308.463098	19.095437	-0.048366	1.230666
263.954574	300.760576	19.100442	-0.048360	1.221808
263.884584	293.095486	19.105447	-0.048341	1.212916
263.750287	285.427732	19.110451	-0.048311	1.203943
263.884952	277.749392	19.115456	-0.048331	1.194944
263.663093	270.105984	19.120461	-0.048285	1.185845
263.710641	262.444988	19.125466	-0.048288	1.176710
263.929725	254.756926	19.130471	-0.048324	1.167507
263.477641	247.201390	19.135475	-0.048234	1.158252
263.284203	239.566849	19.140480	-0.048193	1.148879
263.312400	231.910535	19.145485	-0.048193	1.139450
263.241489	224.291500	19.150490	-0.048175	1.129967
263.274148	216.677495	19.155495	-0.048176	1.120432
263.041240	209.107024	19.160499	-0.048127	1.110813
263.000847	201.511290	19.165504	-0.048115	1.101120
263.124379	193.900206	19.170509	-0.048132	1.091358
263.002326	186.341624	19.175514	-0.048104	1.081520
262.872519	178.798317	19.180519	-0.048075	1.071611
262.740170	171.239762	19.185523	-0.048045	1.061588
262.709440	163.705243	19.190528	-0.048035	1.051525
262.668951	156.166830	19.195533	-0.048022	1.041358
262.773643	148.624016	19.200538	-0.048036	1.031118
262.505788	141.150464	19.205543	-0.047981	1.020783
262.085319	133.709275	19.210547	-0.047898	1.010349
262.212554	126.200097	19.215552	-0.047916	0.999845
262.021487	118.718704	19.220557	-0.047876	0.989190
261.843379	111.262674	19.225562	-0.047838	0.978459
261.812555	103.807252	19.230567	-0.047827	0.967647
261.720744	96.380847	19.235571	-0.047805	0.956740
261.723532	88.948030	19.240576	-0.047800	0.945722
261.809082	81.529817	19.245581	-0.047811	0.934618
261.539546	74.177197	19.250586	-0.047756	0.923386
261.612642	66.799342	19.255591	-0.047764	0.912069
261.127113	59.735211	19.260595	-0.047669	0.900947