Fri Mar 12 11:14:14 2021


Number of Points = 3626

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.348982	-0.102236	0.000000	-0.000005	0.716762
0.172740	-0.077770	0.005005	0.000028	0.716747
0.500049	-0.132712	0.010010	-0.000032	0.716753
0.245492	-0.091971	0.015014	0.000015	0.716744
0.355755	-0.106989	0.020019	-0.000005	0.716753
0.243773	-0.086006	0.025024	0.000016	0.716754
0.156454	-0.072847	0.030029	0.000032	0.716749
0.492956	-0.127060	0.035034	-0.000030	0.716760
0.293588	-0.097214	0.040038	0.000007	0.716748
0.319587	-0.098996	0.045043	0.000003	0.716753
0.343527	-0.102856	0.050048	-0.000001	0.716753
0.281588	-0.095321	0.055053	0.000010	0.716746
0.349718	-0.102952	0.060058	-0.000002	0.716755
0.428370	-0.120895	0.065062	-0.000016	0.716746
0.253328	-0.086669	0.070067	0.000017	0.716752
0.328642	-0.132284	0.075072	0.000003	0.716688
0.466325	-0.283009	0.080077	-0.000022	0.716437
0.512587	-0.288244	0.085082	-0.000031	0.716443
0.247223	-0.244589	0.090086	0.000019	0.716435
0.167243	-0.226706	0.095091	0.000034	0.716442
0.209562	-0.233485	0.100096	0.000026	0.716443
0.200765	-0.234824	0.105101	0.000028	0.716436
0.244613	-0.346648	0.110106	0.000020	0.716230
0.228146	-0.398384	0.115110	0.000024	0.716121
0.390432	-0.422556	0.120115	-0.000006	0.716130
0.545460	-0.451225	0.125120	-0.000035	0.716127
0.481505	-0.440964	0.130125	-0.000023	0.716125
0.396098	-0.523103	0.135130	-0.000006	0.715931
0.128794	-0.504340	0.140134	0.000044	0.715874
0.330243	-0.534978	0.145139	0.000006	0.715884
0.123355	-0.499293	0.150144	0.000045	0.715881
0.295016	-0.623413	0.155149	0.000014	0.715695
0.402730	-0.714706	0.160154	-0.000006	0.715551
0.234905	-0.690820	0.165158	0.000025	0.715539
0.182085	-0.678999	0.170163	0.000035	0.715543
-0.078031	-0.755824	0.175168	0.000084	0.715298
0.028235	-0.811216	0.180173	0.000065	0.715226
0.126626	-0.825979	0.185178	0.000047	0.715231
-0.061188	-0.832794	0.190182	0.000082	0.715150
0.258006	-1.013147	0.195187	0.000023	0.714905
0.189453	-0.999390	0.200192	0.000036	0.714907
-0.087522	-0.962658	0.205197	0.000088	0.714882
-0.115203	-1.095752	0.210202	0.000093	0.714607
-0.077829	-1.105465	0.215206	0.000086	0.714601
-0.024648	-1.114024	0.220211	0.000077	0.714602
0.130434	-1.307836	0.225216	0.000048	0.714272
0.068637	-1.298701	0.230221	0.000060	0.714267
-0.041465	-1.312429	0.235226	0.000081	0.714201
-0.224634	-1.401862	0.240230	0.000115	0.713958
-0.114693	-1.419396	0.245235	0.000095	0.713961
0.075843	-1.539642	0.250240	0.000060	0.713789
-0.144922	-1.575282	0.255245	0.000101	0.713640
-0.181702	-1.566519	0.260250	0.000108	0.713643
-0.377844	-1.679128	0.265254	0.000145	0.713349
-0.120341	-1.722760	0.270259	0.000097	0.713353
-0.141614	-1.809392	0.275264	0.000102	0.713173
-0.340364	-1.854339	0.280269	0.000139	0.713013
-0.198087	-1.905640	0.285274	0.000113	0.712961
-0.518938	-1.979264	0.290278	0.000173	0.712700
-0.333016	-2.010498	0.295283	0.000139	0.712703
-0.357029	-2.149191	0.300288	0.000143	0.712418
-0.398946	-2.162126	0.305293	0.000151	0.712377
-0.606665	-2.220112	0.310298	0.000190	0.712187
-1.824756	-2.057188	0.315302	0.000417	0.712079
-1.852786	-2.076464	0.320307	0.000423	0.712030
-2.224660	-2.144927	0.325312	0.000492	0.711761
-2.518592	-2.095945	0.330317	0.000547	0.711753
-2.631522	-2.138207	0.335322	0.000569	0.711629
-3.640852	-2.049252	0.340326	0.000757	0.711447
-3.619107	-2.051941	0.345331	0.000753	0.711449
-3.653254	-2.084112	0.350336	0.000760	0.711372
-4.525361	-2.052036	0.355341	0.000922	0.711125
-3.968941	-2.144410	0.360346	0.000819	0.711138
-4.836606	-1.994710	0.365350	0.000981	0.711128
-4.811773	-2.103106	0.370355	0.000976	0.710920
-4.785964	-2.134749	0.375360	0.000972	0.710866
-5.409442	-2.026799	0.380365	0.001088	0.710859
-5.131028	-2.087738	0.385370	0.001037	0.710836
-5.873650	-2.111695	0.390374	0.001175	0.710523
-5.955794	-2.094934	0.395379	0.001191	0.710527
-6.093205	-2.069926	0.400384	0.001217	0.710527
-6.128057	-2.066634	0.405389	0.001223	0.710521
-6.335563	-2.172362	0.410394	0.001262	0.710235
-7.145697	-2.042975	0.415398	0.001413	0.710205
-7.225856	-2.024459	0.420403	0.001428	0.710213
-6.713984	-2.115706	0.425408	0.001333	0.710212
-7.228992	-2.078710	0.430413	0.001430	0.710102
-7.891969	-2.066755	0.435418	0.001553	0.709890
-7.558633	-2.130441	0.440422	0.001492	0.709881
-8.052492	-2.039371	0.445427	0.001584	0.709886
-7.843291	-2.075860	0.450432	0.001545	0.709887
-7.781801	-2.130490	0.455437	0.001534	0.709800
-8.589387	-2.091269	0.460442	0.001684	0.709590
-8.594049	-2.093977	0.465446	0.001686	0.709582
-8.971654	-2.025146	0.470451	0.001756	0.709585
-8.570311	-2.094318	0.475456	0.001682	0.709589
-8.611877	-2.090644	0.480461	0.001690	0.709581
-9.238786	-2.138159	0.485466	0.001807	0.709262
-9.613995	-2.076503	0.490470	0.001877	0.709251
-9.654290	-2.067982	0.495475	0.001885	0.709253
-9.720723	-2.052658	0.500480	0.001897	0.709260
-9.855263	-2.034128	0.505485	0.001922	0.709248
-9.570951	-2.093171	0.510490	0.001870	0.709231
-10.299373	-2.106096	0.515494	0.002006	0.708945
-10.831255	-2.009300	0.520499	0.002105	0.708948
-10.628490	-2.044606	0.525504	0.002067	0.708949
-10.587616	-2.054256	0.530509	0.002060	0.708944
-10.689459	-2.032427	0.535514	0.002079	0.708951
-10.464851	-2.075018	0.540518	0.002038	0.708945
-10.604002	-2.161337	0.545523	0.002064	0.708722
-11.647713	-2.020200	0.550528	0.002259	0.708632
-11.627381	-2.026070	0.555533	0.002255	0.708627
-10.961860	-2.139451	0.560538	0.002131	0.708637
-11.478112	-2.051050	0.565542	0.002228	0.708629
-11.843035	-1.984555	0.570547	0.002296	0.708632
-11.356512	-2.099545	0.575552	0.002206	0.708575
-12.232844	-2.059789	0.580557	0.002369	0.708341
-12.276675	-2.048925	0.585562	0.002377	0.708346
-12.726028	-1.972055	0.590566	0.002461	0.708340
-12.193646	-2.065255	0.595571	0.002363	0.708342
-12.372256	-2.033368	0.600576	0.002396	0.708342
-12.670458	-1.981647	0.605581	0.002452	0.708339
-12.001630	-2.174374	0.610586	0.002328	0.708191
-13.277519	-2.040129	0.615590	0.002565	0.708004
-13.383047	-2.020957	0.620595	0.002585	0.708004
-13.276984	-2.037356	0.625600	0.002566	0.708008
-13.397920	-2.018863	0.630605	0.002589	0.708002
-13.195662	-2.050578	0.635610	0.002551	0.708010
-13.325988	-2.031151	0.640614	0.002576	0.708002
-13.340881	-2.123620	0.645619	0.002579	0.707811
-14.425868	-1.989801	0.650624	0.002781	0.707691
-14.288116	-2.017064	0.655629	0.002756	0.707685
-13.862892	-2.086733	0.660634	0.002677	0.707696
-14.207954	-2.029146	0.665638	0.002741	0.707688
-14.321185	-2.007782	0.670643	0.002763	0.707690
-13.895246	-2.080498	0.675648	0.002684	0.707696
-14.159375	-2.153203	0.680653	0.002733	0.707455
-15.305333	-1.988993	0.685658	0.002947	0.707374
-15.172377	-2.016840	0.690662	0.002922	0.707365
-14.709688	-2.098132	0.695667	0.002836	0.707367
-14.977443	-2.049614	0.700672	0.002886	0.707368
-15.364619	-1.982844	0.705677	0.002959	0.707363
-14.892200	-2.061514	0.710682	0.002871	0.707374
-15.045781	-2.145505	0.715686	0.002900	0.707150
-16.187553	-1.979648	0.720691	0.003113	0.707074
-15.709449	-2.064856	0.725696	0.003024	0.707073
-15.739542	-2.061616	0.730701	0.003030	0.707069
-15.917437	-2.026083	0.735706	0.003063	0.707076
-15.976712	-2.018030	0.740710	0.003074	0.707070
-15.722142	-2.061255	0.745715	0.003027	0.707074
-16.190792	-2.134622	0.750720	0.003115	0.706759
-17.038868	-1.991985	0.755725	0.003273	0.706741
-16.734432	-2.042779	0.760730	0.003217	0.706747
-16.376091	-2.110954	0.765734	0.003150	0.706738
-17.014255	-1.995009	0.770739	0.003269	0.706742
-16.673775	-2.052967	0.775744	0.003206	0.706747
-16.461915	-2.118385	0.780749	0.003167	0.706691
-17.536654	-2.050335	0.785754	0.003367	0.706443
-17.829164	-2.003423	0.790758	0.003422	0.706432
-17.768326	-2.013282	0.795763	0.003411	0.706433
-17.254733	-2.101169	0.800768	0.003316	0.706440
-17.833741	-2.001205	0.805773	0.003424	0.706433
-17.484231	-2.059415	0.810778	0.003359	0.706441
-17.359693	-2.112868	0.815782	0.003336	0.706377
-18.604994	-2.019127	0.820787	0.003568	0.706119
-18.705338	-1.998896	0.825792	0.003587	0.706123
-18.769090	-1.989808	0.830797	0.003599	0.706118
-18.306648	-2.068036	0.835802	0.003513	0.706126
-18.497608	-2.036621	0.840806	0.003549	0.706120
-18.756423	-1.990238	0.845811	0.003597	0.706120
-18.340002	-2.060650	0.850816	0.003520	0.706128
-18.994600	-2.073516	0.855821	0.003642	0.705867
-19.358514	-2.010880	0.860826	0.003710	0.705862
-19.056738	-2.066719	0.865830	0.003654	0.705857
-19.211214	-2.039283	0.870835	0.003683	0.705856
-19.235959	-2.032374	0.875840	0.003688	0.705861
-18.973139	-2.083092	0.880845	0.003640	0.705852
-18.840633	-2.190826	0.885850	0.003615	0.705683
-20.637891	-1.952081	0.890854	0.003950	0.705518
-20.181866	-2.033245	0.895859	0.003865	0.705518
-19.829884	-2.093107	0.900864	0.003800	0.705523
-20.414731	-1.992286	0.905869	0.003909	0.705516
-20.120516	-2.039096	0.910874	0.003855	0.705527
-20.034661	-2.060477	0.915878	0.003839	0.705514
-20.387972	-2.106030	0.920883	0.003905	0.705295
-21.287542	-1.988455	0.925888	0.004073	0.705208
-21.101646	-2.025418	0.930893	0.004038	0.705200
-20.635963	-2.103266	0.935898	0.003952	0.705210
-21.259538	-1.994644	0.940902	0.004068	0.705204
-21.296320	-1.987956	0.945907	0.004075	0.705204
-20.757680	-2.082066	0.950912	0.003975	0.705207
-21.418640	-2.080088	0.955917	0.004099	0.704974
-22.124861	-1.997887	0.960922	0.004231	0.704885
-21.754181	-2.067870	0.965926	0.004162	0.704877
-21.753930	-2.067125	0.970931	0.004162	0.704878
-22.141457	-1.995582	0.975936	0.004234	0.704882
-21.995897	-2.028609	0.980941	0.004208	0.704868
-21.388839	-2.131354	0.985946	0.004095	0.704878
-22.306592	-2.096823	0.990950	0.004266	0.704618
-22.776036	-2.031942	0.995955	0.004354	0.704579
-22.656925	-2.050645	1.000960	0.004332	0.704584
-22.633503	-2.060035	1.005965	0.004328	0.704573
-22.704369	-2.042002	1.010970	0.004341	0.704583
-22.615828	-2.060716	1.015974	0.004325	0.704577
-22.367881	-2.142632	1.020979	0.004279	0.704500
-23.622449	-2.039845	1.025984	0.004513	0.704256
-23.587422	-2.050837	1.030989	0.004507	0.704246
-23.290104	-2.100267	1.035994	0.004451	0.704253
-23.465224	-2.071780	1.040998	0.004484	0.704247
-23.603626	-2.047168	1.046003	0.004510	0.704246
-23.592094	-2.043789	1.051008	0.004508	0.704257
-23.823992	-2.077183	1.056013	0.004552	0.704105
-24.566304	-2.024978	1.061018	0.004690	0.703943
-24.069579	-2.114878	1.066022	0.004598	0.703940
-24.357860	-2.064588	1.071027	0.004652	0.703937
-24.723016	-1.995059	1.076032	0.004720	0.703946
-24.672687	-2.007616	1.081037	0.004711	0.703938
-24.175835	-2.091810	1.086042	0.004619	0.703946
-24.360317	-2.144844	1.091046	0.004654	0.703773
-25.726115	-1.976096	1.096051	0.004908	0.703621
-25.196714	-2.065363	1.101056	0.004810	0.703631
-25.338965	-2.046136	1.106061	0.004837	0.703618
-25.707454	-1.973925	1.111066	0.004905	0.703631
-25.528796	-2.008857	1.116070	0.004872	0.703624
-25.108310	-2.082535	1.121075	0.004794	0.703626
-25.141653	-2.138651	1.126080	0.004801	0.703501
-26.368067	-2.003420	1.131085	0.005029	0.703332
-25.910434	-2.079933	1.136090	0.004944	0.703341
-26.300593	-2.014221	1.141094	0.005017	0.703333
-26.417187	-1.994771	1.146099	0.005039	0.703330
-26.088282	-2.051890	1.151104	0.004978	0.703333
-26.356808	-2.008831	1.156109	0.005029	0.703322
-26.256025	-2.109126	1.161114	0.005010	0.703156
-27.343237	-1.993565	1.166118	0.005213	0.702997
-27.111353	-2.035049	1.171123	0.005170	0.702996
-27.184198	-2.018915	1.176128	0.005184	0.703002
-27.380977	-1.987718	1.181133	0.005221	0.702994
-26.950274	-2.059318	1.186138	0.005141	0.703004
-27.131233	-2.029975	1.191142	0.005175	0.702997
-27.640733	-1.965624	1.196147	0.005270	0.702943
-27.959207	-2.036430	1.201152	0.005329	0.702685
-27.855326	-2.057177	1.206157	0.005310	0.702680
-28.340162	-1.967238	1.211162	0.005401	0.702687
-28.307773	-1.974852	1.216166	0.005395	0.702682
-28.001635	-2.030039	1.221171	0.005338	0.702681
-28.065857	-2.014788	1.226176	0.005350	0.702688
-28.325196	-1.972935	1.231181	0.005399	0.702678
-28.272211	-2.100540	1.236186	0.005389	0.702439
-29.062874	-1.998115	1.241190	0.005537	0.702361
-29.075122	-1.995954	1.246195	0.005539	0.702360
-28.781831	-2.045455	1.251200	0.005485	0.702365
-29.109881	-1.990652	1.256205	0.005546	0.702357
-28.819659	-2.038215	1.261210	0.005493	0.702365
-28.717917	-2.058773	1.266214	0.005474	0.702360
-29.198298	-2.101987	1.271219	0.005564	0.702099
-29.648598	-2.036227	1.276224	0.005648	0.702069
-30.106398	-1.957282	1.281229	0.005733	0.702063
-29.397152	-2.079295	1.286234	0.005601	0.702072
-29.426575	-2.077429	1.291238	0.005607	0.702064
-30.094924	-1.956348	1.296243	0.005732	0.702068
-29.656569	-2.055797	1.301248	0.005651	0.702024
-30.524220	-2.045664	1.306253	0.005812	0.701731
-30.574645	-2.032376	1.311258	0.005822	0.701739
-30.931801	-1.971297	1.316262	0.005889	0.701733
-30.638910	-2.024433	1.321267	0.005834	0.701731
-30.285149	-2.083641	1.326272	0.005769	0.701738
-30.925882	-1.973655	1.331277	0.005888	0.701729
-30.683098	-2.027075	1.336282	0.005843	0.701708
-31.106715	-2.090497	1.341286	0.005923	0.701427
-31.576840	-2.007074	1.346291	0.006010	0.701425
-31.588996	-2.000457	1.351296	0.006013	0.701434
-31.474642	-2.025921	1.356301	0.005992	0.701423
-31.482486	-2.020806	1.361306	0.005994	0.701430
-31.452861	-2.028270	1.366310	0.005988	0.701425
-31.495589	-2.051052	1.371315	0.005997	0.701363
-32.148149	-2.055888	1.376320	0.006118	0.701117
-32.520240	-1.993913	1.381325	0.006188	0.701108
-32.466300	-1.999663	1.386330	0.006178	0.701115
-32.015040	-2.081003	1.391334	0.006094	0.701113
-32.318746	-2.026713	1.396339	0.006151	0.701113
-32.206897	-2.044832	1.401344	0.006131	0.701116
-32.188810	-2.104684	1.406349	0.006127	0.701001
-33.093656	-2.009575	1.411354	0.006296	0.700866
-33.142829	-2.003140	1.416358	0.006306	0.700861
-33.217523	-1.989881	1.421363	0.006320	0.700860
-32.936080	-2.035816	1.426368	0.006268	0.700868
-33.140396	-2.004296	1.431373	0.006306	0.700858
-33.049131	-2.015162	1.436378	0.006289	0.700868
-33.266940	-2.127428	1.441382	0.006330	0.700561
-33.953101	-2.024917	1.446387	0.006458	0.700521
-33.969600	-2.018185	1.451392	0.006461	0.700528
-33.856321	-2.042374	1.456397	0.006441	0.700519
-33.944044	-2.023095	1.461402	0.006457	0.700526
-34.194661	-1.979580	1.466406	0.006504	0.700523
-34.055730	-2.040721	1.471411	0.006478	0.700449
-34.411187	-2.092364	1.476416	0.006545	0.700215
-34.673496	-2.052420	1.481421	0.006594	0.700201
-34.937752	-1.998967	1.486426	0.006643	0.700213
-34.554179	-2.068008	1.491430	0.006572	0.700211
-34.705924	-2.043163	1.496435	0.006601	0.700206
-34.934383	-1.998095	1.501440	0.006644	0.700215
-34.748892	-2.139164	1.506445	0.006609	0.699995
-35.547171	-2.049141	1.511450	0.006758	0.699888
-35.530366	-2.053314	1.516454	0.006755	0.699886
-35.697060	-2.025801	1.521459	0.006787	0.699881
-35.233079	-2.103914	1.526464	0.006701	0.699889
-35.522416	-2.056913	1.531469	0.006755	0.699880
-35.650038	-2.069792	1.536474	0.006779	0.699807
-36.359134	-2.050372	1.541478	0.006911	0.699589
-36.218617	-2.077915	1.546483	0.006885	0.699583
-36.524197	-2.019671	1.551488	0.006942	0.699591
-36.838179	-1.965696	1.556493	0.007001	0.699586
-36.506629	-2.019888	1.561498	0.006939	0.699596
-36.607894	-2.003119	1.566502	0.006959	0.699592
-36.625422	-2.035462	1.571507	0.006962	0.699520
-37.238566	-2.053434	1.576512	0.007076	0.699261
-37.155009	-2.072201	1.581517	0.007061	0.699252
-37.502707	-2.005448	1.586522	0.007126	0.699262
-37.211979	-2.058126	1.591526	0.007072	0.699259
-37.223253	-2.058251	1.596531	0.007075	0.699255
-37.497380	-2.004465	1.601536	0.007126	0.699264
-37.214571	-2.120401	1.606541	0.007074	0.699130
-37.959959	-2.074575	1.611546	0.007213	0.698953
-38.065450	-2.055475	1.616550	0.007233	0.698953
-38.645296	-1.955693	1.621555	0.007341	0.698945
-37.982544	-2.068730	1.626560	0.007218	0.698955
-38.046900	-2.061883	1.631565	0.007230	0.698945
-38.368294	-2.001128	1.636570	0.007290	0.698952
-38.406436	-2.096005	1.641574	0.007297	0.698745
-39.264590	-2.000989	1.646579	0.007457	0.698626
-38.953619	-2.051214	1.651584	0.007400	0.698636
-39.115969	-2.026234	1.656589	0.007430	0.698628
-38.966622	-2.050320	1.661594	0.007403	0.698632
-39.034640	-2.037557	1.666598	0.007416	0.698633
-39.201650	-2.009750	1.671603	0.007447	0.698629
-38.955605	-2.161099	1.676608	0.007401	0.698410
-39.739601	-2.055830	1.681613	0.007548	0.698339
-39.896893	-2.025303	1.686618	0.007577	0.698343
-39.516446	-2.092028	1.691622	0.007507	0.698345
-39.976909	-2.012034	1.696627	0.007593	0.698340
-39.886525	-2.023878	1.701632	0.007576	0.698349
-39.949532	-2.063660	1.706637	0.007588	0.698244
-40.740665	-2.039470	1.711642	0.007736	0.698006
-40.301561	-2.117004	1.716646	0.007654	0.698007
-40.971339	-2.000517	1.721651	0.007779	0.698000
-40.733683	-2.037825	1.726656	0.007735	0.698010
-40.636123	-2.060272	1.731661	0.007717	0.697999
-40.865204	-2.015369	1.736666	0.007760	0.698007
-40.784115	-2.096242	1.741670	0.007745	0.697872
-41.960717	-1.974592	1.746675	0.007964	0.697691
-41.403797	-2.069538	1.751680	0.007861	0.697700
-41.529720	-2.053119	1.756685	0.007885	0.697687
-41.451974	-2.063901	1.761690	0.007871	0.697693
-41.261527	-2.096051	1.766694	0.007835	0.697696
-41.732161	-2.015962	1.771699	0.007923	0.697688
-41.614751	-2.142761	1.776704	0.007902	0.697472
-42.769272	-1.988321	1.781709	0.008117	0.697366
-42.831855	-1.975186	1.786714	0.008129	0.697370
-42.369812	-2.057161	1.791718	0.008043	0.697370
-42.314544	-2.070068	1.796723	0.008033	0.697364
-42.566350	-2.019886	1.801728	0.008080	0.697374
-42.580346	-2.020630	1.806733	0.008083	0.697367
-42.453923	-2.130789	1.811738	0.008060	0.697188
-43.414992	-2.014813	1.816742	0.008239	0.697074
-43.232032	-2.050226	1.821747	0.008205	0.697068
-43.003506	-2.085915	1.826752	0.008163	0.697078
-43.333551	-2.031049	1.831757	0.008225	0.697069
-43.304991	-2.032794	1.836762	0.008219	0.697076
-43.330672	-2.027889	1.841766	0.008224	0.697076
-43.941195	-2.076053	1.846771	0.008338	0.696755
-43.879759	-2.088257	1.851776	0.008327	0.696752
-44.336361	-2.012995	1.856781	0.008413	0.696739
-44.016821	-2.065649	1.861786	0.008353	0.696747
-43.931637	-2.079525	1.866790	0.008338	0.696749
-44.408054	-1.997857	1.871795	0.008427	0.696742
-44.044603	-2.085028	1.876800	0.008359	0.696696
-44.769612	-2.083061	1.881805	0.008495	0.696436
-45.014595	-2.038042	1.886810	0.008540	0.696438
-44.876685	-2.060061	1.891814	0.008515	0.696443
-44.794821	-2.077899	1.896819	0.008500	0.696436
-44.634459	-2.101588	1.901824	0.008470	0.696445
-45.132423	-2.016265	1.906829	0.008563	0.696438
-44.908560	-2.149384	1.911834	0.008522	0.696247
-45.825514	-2.045663	1.916838	0.008693	0.696124
-46.136148	-1.991878	1.921843	0.008751	0.696121
-45.661627	-2.072414	1.926848	0.008663	0.696128
-45.817225	-2.048810	1.931853	0.008692	0.696119
-45.835872	-2.041870	1.936858	0.008696	0.696126
-46.000147	-2.013237	1.941862	0.008727	0.696124
-45.999298	-2.103090	1.946867	0.008727	0.695941
-46.469787	-2.053250	1.951872	0.008815	0.695871
-46.661711	-2.021672	1.956877	0.008851	0.695865
-46.446818	-2.058382	1.961882	0.008811	0.695868
-46.381493	-2.068182	1.966886	0.008799	0.695871
-46.684955	-2.016478	1.971891	0.008856	0.695866
-46.750176	-2.034035	1.976896	0.008868	0.695805
-47.296305	-2.072588	1.981901	0.008970	0.695527
-47.450187	-2.043361	1.986906	0.008999	0.695530
-47.727066	-1.993148	1.991910	0.009051	0.695532
-47.293810	-2.072635	1.996915	0.008970	0.695527
-47.552733	-2.023282	2.001920	0.009019	0.695532
-47.315177	-2.128028	2.011917	0.008975	0.695404
-48.636826	-1.982721	2.021914	0.009222	0.695218
-48.263729	-2.050124	2.031910	0.009153	0.695216
-48.609718	-1.987143	2.041907	0.009218	0.695217
-48.390920	-2.025566	2.051904	0.009178	0.695217
-48.570075	-1.991965	2.061901	0.009211	0.695220
-48.374897	-2.027322	2.071898	0.009176	0.695218
-48.441320	-1.965869	2.081894	0.009188	0.695318
-47.573090	-2.016507	2.091891	0.009027	0.695530
-47.479486	-2.031716	2.101888	0.009010	0.695532
-47.565707	-2.015420	2.111885	0.009027	0.695533
-47.476716	-2.029998	2.121882	0.009011	0.695534
-47.392185	-2.046191	2.131878	0.008996	0.695531
-47.561127	-2.015177	2.141875	0.009028	0.695532
-47.419336	-2.039556	2.151872	0.009002	0.695533
-47.055906	-1.990883	2.161869	0.008935	0.695763
-46.694872	-2.001125	2.171866	0.008868	0.695873
-46.433247	-2.048220	2.181862	0.008820	0.695871
-46.603353	-2.018262	2.191859	0.008852	0.695869
-46.435466	-2.046836	2.201856	0.008821	0.695871
-46.051895	-2.007594	2.211853	0.008750	0.696090
-45.895300	-2.017801	2.221850	0.008722	0.696125
-45.742984	-2.045703	2.231846	0.008694	0.696123
-45.990154	-1.998553	2.241843	0.008740	0.696128
-45.208041	-1.984194	2.251840	0.008595	0.696441
-45.100237	-2.002011	2.261837	0.008576	0.696443
-44.853981	-2.045904	2.271834	0.008530	0.696442
-44.870139	-1.989686	2.281830	0.008534	0.696549
-44.161104	-2.019581	2.291827	0.008402	0.696745
-44.022151	-2.042569	2.301824	0.008377	0.696748
-44.246295	-2.001059	2.311821	0.008419	0.696750
-43.282825	-2.051382	2.321818	0.008240	0.696997
-43.243800	-2.018694	2.331814	0.008234	0.697077
-43.105444	-2.043531	2.341811	0.008208	0.697075
-43.268516	-2.007238	2.351808	0.008239	0.697089
-42.535922	-1.998358	2.361805	0.008103	0.697372
-42.237610	-2.051534	2.371802	0.008048	0.697371
-42.475127	-2.009672	2.381798	0.008093	0.697369
-42.298164	-1.952175	2.391795	0.008061	0.697550
-41.337809	-2.051044	2.401792	0.007882	0.697696
-41.558119	-2.010986	2.411789	0.007924	0.697697
-41.256969	-2.063593	2.421786	0.007868	0.697698
-40.655131	-2.020005	2.431782	0.007757	0.698004
-40.424307	-2.059990	2.441779	0.007714	0.698006
-40.406955	-2.061554	2.451776	0.007712	0.698008
-40.449913	-2.007884	2.461773	0.007720	0.698100
-39.453821	-2.064302	2.471770	0.007535	0.698346
-39.643738	-2.030627	2.481766	0.007571	0.698344
-39.768648	-2.007893	2.491763	0.007595	0.698344
-39.150124	-2.013760	2.501760	0.007480	0.698556
-39.013952	-1.997268	2.511757	0.007455	0.698638
-38.729117	-2.048459	2.521754	0.007403	0.698636
-38.840093	-1.976349	2.531750	0.007424	0.698741
-37.856651	-2.047964	2.541747	0.007241	0.698951
-38.087818	-2.006704	2.551744	0.007285	0.698950
-37.951762	-2.030360	2.561741	0.007260	0.698950
-37.322096	-2.004450	2.571738	0.007143	0.699230
-36.989531	-2.050108	2.581734	0.007082	0.699257
-36.914344	-2.061061	2.591731	0.007068	0.699261
-36.873946	-2.018016	2.601728	0.007061	0.699362
-36.165742	-2.029662	2.611725	0.006930	0.699594
-36.044323	-2.051362	2.621722	0.006908	0.699593
-36.354410	-1.996722	2.631718	0.006966	0.699590
-35.591317	-2.011569	2.641715	0.006825	0.699835
-35.442262	-2.011084	2.651712	0.006797	0.699889
-35.120856	-2.068872	2.661709	0.006738	0.699887
-35.196868	-2.008794	2.671706	0.006753	0.699981
-34.501967	-2.019576	2.681702	0.006624	0.700209
-34.322463	-2.050824	2.691699	0.006591	0.700210
-34.638944	-1.992350	2.701696	0.006650	0.700213
-33.865619	-1.994718	2.711693	0.006507	0.700487
-33.691168	-2.004440	2.721690	0.006475	0.700529
-33.506878	-2.037505	2.731686	0.006441	0.700528
-33.240498	-2.020861	2.741683	0.006392	0.700657
-32.639860	-2.022388	2.751680	0.006281	0.700870
-32.594884	-2.029915	2.761677	0.006273	0.700870
-32.735242	-2.005896	2.771674	0.006300	0.700867
-32.211801	-1.995514	2.781670	0.006203	0.701076
-31.856927	-2.038972	2.791667	0.006137	0.701115
-31.910240	-2.028431	2.801664	0.006148	0.701116
-31.451984	-2.038650	2.811661	0.006063	0.701260
-31.033028	-2.030921	2.821658	0.005985	0.701426
-31.238231	-1.994029	2.831654	0.006024	0.701425
-31.044076	-2.012175	2.841651	0.005988	0.701458
-30.306178	-2.006920	2.851648	0.005851	0.701734
-29.923435	-2.072203	2.861645	0.005781	0.701739
-30.206020	-2.021823	2.871642	0.005834	0.701738
-29.657928	-2.017667	2.881638	0.005732	0.701943
-29.226311	-2.035370	2.891635	0.005652	0.702062
-29.472929	-1.988506	2.901632	0.005699	0.702067
-29.200312	-2.006676	2.911629	0.005649	0.702127
-28.419964	-2.028602	2.921626	0.005504	0.702363
-28.378556	-2.035878	2.931622	0.005497	0.702362
-28.416709	-2.028504	2.941619	0.005504	0.702362
-27.882321	-2.014691	2.951616	0.005405	0.702582
-27.623934	-2.009647	2.961613	0.005358	0.702684
-27.716786	-1.992133	2.971610	0.005375	0.702685
-27.440029	-1.996042	2.981606	0.005324	0.702776
-26.669377	-2.025291	2.991603	0.005181	0.702994
-26.662504	-2.026062	3.001600	0.005181	0.702993
-26.460813	-2.059440	3.011597	0.005144	0.702998
-26.062822	-1.998595	3.021594	0.005070	0.703263
-25.737399	-2.021709	3.031590	0.005010	0.703332
-25.714365	-2.025903	3.041587	0.005006	0.703331
-25.501005	-2.039680	3.051584	0.004967	0.703379
-25.039798	-1.999519	3.061581	0.004882	0.703625
-24.816527	-2.038019	3.071578	0.004841	0.703627
-24.869327	-2.029544	3.081574	0.004851	0.703624
-24.218452	-2.032064	3.091571	0.004730	0.703852
-23.908204	-2.042211	3.101568	0.004673	0.703942
-23.882353	-2.045473	3.111565	0.004669	0.703944
-24.113174	-1.986972	3.121562	0.004712	0.703978
-23.031524	-2.044289	3.131558	0.004511	0.704250
-22.909240	-2.065791	3.141555	0.004489	0.704250
-23.120659	-2.025201	3.151552	0.004529	0.704254
-22.754075	-2.000502	3.161549	0.004461	0.704435
-22.002262	-2.060631	3.171546	0.004322	0.704583
-22.272024	-2.013324	3.181542	0.004372	0.704580
-22.180296	-2.029572	3.191539	0.004356	0.704580
-21.582561	-1.993233	3.201536	0.004245	0.704866
-21.419163	-2.015273	3.211533	0.004215	0.704880
-21.253342	-2.045040	3.221530	0.004185	0.704878
-20.962748	-2.003642	3.231526	0.004131	0.705065
-20.534250	-2.012619	3.241523	0.004052	0.705200
-20.482943	-2.019059	3.251520	0.004043	0.705204
-20.370286	-2.032322	3.261517	0.004022	0.705217
-19.568185	-2.026061	3.271514	0.003874	0.705516
-19.449649	-2.046582	3.281510	0.003852	0.705517
-19.310598	-2.072120	3.291507	0.003827	0.705514
-19.369667	-2.012623	3.301504	0.003838	0.705612
-18.527717	-2.039877	3.311501	0.003682	0.705858
-18.542849	-2.038863	3.321498	0.003685	0.705853
-18.572918	-2.034485	3.331494	0.003691	0.705850
-18.132099	-2.016154	3.341491	0.003610	0.706044
-17.681418	-2.059266	3.351488	0.003526	0.706118
-17.944792	-2.010268	3.361485	0.003576	0.706121
-17.643428	-2.016222	3.371482	0.003520	0.706216
-16.786879	-2.061715	3.381478	0.003361	0.706431
-16.895106	-2.041618	3.391475	0.003382	0.706431
-16.947438	-2.031213	3.401472	0.003392	0.706433
-16.487954	-1.985815	3.411469	0.003307	0.706687
-16.087860	-2.030222	3.421466	0.003233	0.706740
-16.087890	-2.030657	3.431462	0.003234	0.706738
-15.840621	-2.000577	3.441459	0.003188	0.706886
-14.861123	-2.082587	3.451456	0.003007	0.707071
-14.984227	-2.059567	3.461453	0.003030	0.707073
-14.978871	-2.059600	3.471450	0.003029	0.707073
-14.564693	-2.024421	3.481446	0.002953	0.707291
-14.402379	-2.014306	3.491443	0.002923	0.707369
-14.165899	-2.054952	3.501440	0.002880	0.707371
-14.131840	-2.018154	3.511437	0.002874	0.707456
-13.125587	-2.079133	3.521434	0.002687	0.707692
-13.523372	-2.010075	3.531430	0.002761	0.707687
-13.432743	-2.024138	3.541427	0.002745	0.707691
-12.643653	-2.043365	3.551424	0.002599	0.707933
-12.531907	-2.025485	3.561421	0.002578	0.708008
-12.255719	-2.074686	3.571418	0.002528	0.708007
-12.677835	-1.968627	3.581414	0.002607	0.708068
-11.691145	-2.007207	3.591411	0.002423	0.708342
-11.382942	-2.060671	3.601408	0.002367	0.708344
-11.620511	-2.017133	3.611405	0.002411	0.708345
-10.807056	-2.067928	3.621402	0.002260	0.708533
-10.841719	-2.012955	3.631398	0.002267	0.708630
-10.570316	-2.060912	3.641395	0.002217	0.708630
-10.678522	-2.024082	3.651392	0.002238	0.708664
-9.786653	-2.040325	3.661389	0.002072	0.708948
-9.691245	-2.055742	3.671386	0.002055	0.708951
-9.707562	-2.053278	3.681382	0.002059	0.708949
-9.534586	-2.026576	3.691379	0.002027	0.709063
-8.808510	-2.059309	3.701376	0.001892	0.709255
-8.778350	-2.063526	3.711373	0.001887	0.709257
-8.840293	-2.053126	3.721370	0.001899	0.709255
-8.104488	-2.045683	3.731366	0.001763	0.709531
-7.675553	-2.095377	3.741363	0.001684	0.709583
-7.712025	-2.086508	3.751360	0.001691	0.709587
-7.630868	-2.100088	3.761357	0.001676	0.709588
-7.230991	-2.032588	3.771354	0.001602	0.709864
-7.139751	-2.038622	3.781350	0.001586	0.709884
-6.870640	-2.088277	3.791347	0.001536	0.709879
-6.841889	-2.020817	3.801344	0.001531	0.710024
-5.797252	-2.113695	3.811341	0.001337	0.710209
-6.128921	-2.053626	3.821338	0.001400	0.710210
-6.125554	-2.054241	3.831334	0.001400	0.710209
-5.488832	-2.036684	3.841331	0.001281	0.710470
-5.350318	-2.032626	3.851328	0.001256	0.710526
-5.042359	-2.086543	3.861325	0.001199	0.710527
-4.937975	-2.055660	3.871322	0.001180	0.710625
-3.893284	-2.119959	3.881318	0.000986	0.710867
-4.146474	-2.075561	3.891315	0.001034	0.710865
-4.257666	-2.054313	3.901312	0.001055	0.710867
-3.861219	-2.073141	3.911309	0.000982	0.710969
-3.286412	-2.091749	3.921306	0.000876	0.711135
-3.356080	-2.080447	3.931302	0.000889	0.711132
-3.273997	-2.095207	3.941299	0.000874	0.711131
-2.999559	-2.019371	3.951296	0.000824	0.711379
-2.366484	-2.095370	3.961293	0.000706	0.711451
-2.667057	-2.042296	3.971290	0.000763	0.711449
-2.502397	-2.005000	3.981286	0.000733	0.711581
-2.046113	-1.998765	3.991283	0.000648	0.711755
-1.850544	-2.031983	4.001280	0.000612	0.711757
-1.676776	-2.017411	4.011277	0.000580	0.711847
-1.586423	-1.913230	4.021274	0.000564	0.712086
-1.783128	-1.879648	4.031270	0.000601	0.712082
-1.647277	-1.808994	4.041267	0.000576	0.712270
-1.633642	-1.755851	4.051264	0.000574	0.712380
-1.173553	-1.783662	4.061261	0.000489	0.712486
-1.090678	-1.690286	4.071258	0.000474	0.712701
-1.015832	-1.684445	4.081254	0.000461	0.712738
-0.713742	-1.599460	4.091251	0.000405	0.713013
-0.873652	-1.561364	4.101248	0.000435	0.713031
-0.886525	-1.398322	4.111245	0.000438	0.713350
-0.913758	-1.352233	4.121242	0.000444	0.713431
-0.790895	-1.267330	4.131238	0.000421	0.713643
-0.674227	-1.188801	4.141235	0.000400	0.713839
-0.636286	-1.125671	4.151232	0.000393	0.713977
-0.443463	-1.012280	4.161229	0.000358	0.714270
-0.349544	-0.937243	4.171226	0.000341	0.714451
-0.463377	-0.825485	4.181222	0.000362	0.714632
-0.434937	-0.697239	4.191219	0.000358	0.714895
-0.332993	-0.584127	4.201216	0.000339	0.715155
-0.184253	-0.498137	4.211213	0.000312	0.715377
-0.274810	-0.356239	4.221210	0.000329	0.715626
-0.440769	-0.188091	4.231206	0.000360	0.715899
-0.240402	-0.108222	4.241203	0.000324	0.716127
-0.246557	0.050494	4.251200	0.000325	0.716439
0.000000	0.174831	4.261197	0.000280	0.716771
-0.111342	0.824970	4.266202	0.000300	0.718017
0.092776	2.038674	4.271206	0.000262	0.720483
0.428608	3.818049	4.276211	0.000198	0.724095
0.638816	6.170867	4.281216	0.000158	0.728764
1.087567	8.999436	4.286221	0.000073	0.734404
1.488152	12.304696	4.291226	-0.000004	0.740899
1.911129	16.064804	4.296230	-0.000085	0.748207
2.419385	20.229976	4.301235	-0.000182	0.756234
3.006425	24.756830	4.306240	-0.000294	0.764873
3.708486	29.657625	4.311245	-0.000428	0.774139
4.016179	34.959224	4.316250	-0.000488	0.783893
4.499442	40.561571	4.321254	-0.000581	0.794121
5.107743	46.438857	4.326259	-0.000698	0.804743
6.240655	52.507473	4.331264	-0.000913	0.815720
7.450618	58.851600	4.336269	-0.001142	0.827046
8.864745	65.416449	4.341274	-0.001409	0.838654
9.597989	72.309904	4.346278	-0.001550	0.850450
12.114460	79.119820	4.351283	-0.002023	0.862464
12.709483	86.472662	4.356288	-0.002138	0.874643
13.486758	93.966577	4.361293	-0.002288	0.886932
14.400283	101.598245	4.366298	-0.002462	0.899307
15.375111	109.365810	4.371302	-0.002649	0.911742
16.821186	117.177331	4.376307	-0.002923	0.924203
17.548481	125.230602	4.381312	-0.003063	0.936674
18.463401	133.364818	4.386317	-0.003239	0.949149
19.438516	141.568955	4.391322	-0.003425	0.961582
20.538733	149.842748	4.396326	-0.003635	0.973987
22.093859	158.124497	4.401331	-0.003930	0.986362
22.873513	166.604265	4.406336	-0.004080	0.998672
24.009162	175.054068	4.411341	-0.004297	1.010877
24.904430	183.585187	4.416346	-0.004469	1.022990
25.179667	192.266258	4.421350	-0.004526	1.035018
26.109744	200.843480	4.426355	-0.004704	1.046922
26.916310	209.472109	4.431360	-0.004860	1.058731
27.453913	218.172786	4.436365	-0.004965	1.070443
28.851137	226.710619	4.441370	-0.005231	1.082010
31.674613	235.086656	4.446374	-0.005762	1.093562
32.632635	243.778872	4.451379	-0.005945	1.104985
33.288582	252.512543	4.456384	-0.006073	1.116278
33.985466	261.210933	4.461389	-0.006208	1.127422
34.505495	269.950521	4.466394	-0.006311	1.138470
35.599318	278.586908	4.471398	-0.006520	1.149405
36.753448	287.218211	4.476403	-0.006740	1.160243
37.707223	295.839968	4.481408	-0.006923	1.170927
38.532859	304.486855	4.486413	-0.007082	1.181518
39.843225	313.037683	4.491418	-0.007331	1.191999
41.171965	321.574058	4.496422	-0.007584	1.202374
42.168495	330.179985	4.501427	-0.007775	1.212674
42.603162	338.844216	4.506432	-0.007861	1.222845
43.418349	347.461011	4.511437	-0.008018	1.232951
44.104244	356.046862	4.516442	-0.008151	1.242915
44.802416	364.616046	4.521446	-0.008287	1.252782
45.852680	373.110333	4.526451	-0.008487	1.262554
46.756066	381.617156	4.531456	-0.008661	1.272238
47.627281	390.118719	4.536461	-0.008828	1.281835
48.248033	398.646881	4.541466	-0.008949	1.291345
49.110476	407.118463	4.546470	-0.009115	1.300766
50.256484	415.602917	4.551475	-0.009334	1.310186
51.018506	424.126707	4.556480	-0.009481	1.319510
52.535559	432.447765	4.561485	-0.009769	1.328687
53.023785	440.935352	4.566490	-0.009865	1.337795
53.733867	449.347368	4.571494	-0.010002	1.346801
54.543763	457.771961	4.576499	-0.010158	1.355777
55.129448	466.177470	4.581504	-0.010273	1.364635
55.792780	474.602377	4.586509	-0.010401	1.373468
56.496543	482.987903	4.591514	-0.010538	1.382212
57.290193	491.369546	4.596518	-0.010691	1.390912
58.001533	499.745660	4.601523	-0.010828	1.399537
58.733524	508.083671	4.606528	-0.010970	1.408075
59.250901	516.469459	4.611533	-0.011071	1.416573
59.826022	524.808507	4.616538	-0.011184	1.424984
60.323408	533.172337	4.621542	-0.011281	1.433356
60.993884	541.484578	4.626547	-0.011411	1.441658
61.994998	549.732359	4.631552	-0.011603	1.449901
62.360380	558.116826	4.636557	-0.011676	1.458129
62.869861	566.430895	4.641562	-0.011776	1.466265
63.434977	574.787821	4.646566	-0.011887	1.474406
64.134716	583.056024	4.651571	-0.012022	1.482439
64.676359	591.335331	4.656576	-0.012128	1.490413
65.108738	599.652024	4.661581	-0.012214	1.498364
65.718588	607.894932	4.666586	-0.012332	1.506230
65.824758	616.247197	4.671590	-0.012357	1.514081
66.700193	624.439633	4.676595	-0.012525	1.521859
67.293429	632.678044	4.681600	-0.012641	1.529597
68.233593	640.888574	4.686605	-0.012821	1.537323
68.856069	649.142076	4.691610	-0.012942	1.545001
69.399845	657.414451	4.696614	-0.013048	1.552647
70.408505	665.604963	4.701619	-0.013241	1.560249
70.663010	673.883574	4.706624	-0.013294	1.567783
71.182008	682.150312	4.711629	-0.013396	1.575309
72.089929	690.322173	4.716634	-0.013570	1.582770
72.555527	698.568119	4.721638	-0.013662	1.590199
73.288357	706.785075	4.726643	-0.013803	1.597605
73.969345	714.974562	4.731648	-0.013935	1.604945
74.600475	723.211792	4.736653	-0.014058	1.612286
75.093966	731.443873	4.741658	-0.014155	1.619570
75.416743	739.689118	4.746662	-0.014220	1.626809
76.090722	747.950867	4.751667	-0.014350	1.634078
76.748813	756.106755	4.756672	-0.014478	1.641222
77.199726	764.322706	4.761677	-0.014567	1.648357
77.720262	772.521750	4.766682	-0.014669	1.655457
77.897914	780.759991	4.771686	-0.014707	1.662513
78.440709	788.943103	4.776691	-0.014813	1.669542
78.979903	797.112554	4.781696	-0.014919	1.676529
79.494559	805.288859	4.786701	-0.015020	1.683489
79.703664	813.515317	4.791706	-0.015064	1.690422
80.305180	821.674709	4.796710	-0.015181	1.697323
81.163598	829.805647	4.801715	-0.015346	1.704205
81.826670	837.977407	4.806720	-0.015474	1.711068
82.677010	846.137321	4.811725	-0.015638	1.717917
83.025660	854.324588	4.816730	-0.015708	1.724697
83.539573	862.503442	4.821734	-0.015808	1.731464
84.296596	870.658915	4.826739	-0.015955	1.738217
85.083904	878.773487	4.831744	-0.016106	1.744915
85.755931	886.944658	4.836749	-0.016236	1.751617
86.307976	895.115786	4.841754	-0.016344	1.758279
86.892499	903.255629	4.846758	-0.016458	1.764894
87.340543	911.454919	4.851763	-0.016547	1.771515
87.821772	919.624911	4.856768	-0.016641	1.778091
88.382652	927.771956	4.861773	-0.016751	1.784635
88.778528	935.995633	4.866778	-0.016830	1.791196
89.283311	944.159458	4.871782	-0.016929	1.797698
89.830523	952.285718	4.876787	-0.017036	1.804152
90.258721	960.421501	4.881792	-0.017120	1.810577
90.844746	968.575673	4.886797	-0.017234	1.817012
91.123957	976.731452	4.891802	-0.017292	1.823388
91.402111	984.895253	4.896806	-0.017348	1.829748
91.938260	993.036728	4.901811	-0.017453	1.836099
92.297339	1001.167282	4.906816	-0.017525	1.842400
92.659057	1009.320526	4.911821	-0.017598	1.848696
93.075139	1017.467620	4.916826	-0.017680	1.854972
93.604930	1025.576673	4.921830	-0.017784	1.861211
94.280733	1033.694430	4.926835	-0.017915	1.867453
94.451336	1041.890233	4.931840	-0.017951	1.873675
94.957876	1050.002964	4.936845	-0.018051	1.879852
95.343192	1058.124499	4.941850	-0.018128	1.886001
95.776164	1066.258780	4.946854	-0.018213	1.892145
96.135741	1074.408029	4.951859	-0.018285	1.898272
96.661019	1082.490989	4.956864	-0.018388	1.904348
96.918897	1090.656339	4.961869	-0.018441	1.910436
97.471380	1098.764119	4.966874	-0.018549	1.916495
97.811842	1106.876868	4.971878	-0.018618	1.922515
98.121840	1115.022302	4.976883	-0.018680	1.928537
98.292704	1123.169641	4.981888	-0.018717	1.934526
99.229409	1131.207060	4.986893	-0.018897	1.940500
99.706448	1139.329696	4.991898	-0.018990	1.946467
100.000939	1147.504222	4.996902	-0.019050	1.952434
100.634553	1155.605906	5.001907	-0.019173	1.958366
101.137811	1163.675964	5.006912	-0.019272	1.964243
101.613604	1171.780178	5.011917	-0.019366	1.970125
102.292064	1179.872461	5.016922	-0.019497	1.976002
103.061404	1187.925819	5.021926	-0.019645	1.981843
103.565645	1196.057537	5.026931	-0.019744	1.987694
103.812771	1204.212743	5.031936	-0.019795	1.993518
104.361265	1212.305595	5.036941	-0.019902	1.999312
104.804809	1220.402129	5.041946	-0.019990	2.005081
105.175629	1228.531804	5.046950	-0.020064	2.010849
105.531435	1236.661783	5.051955	-0.020135	2.016599
105.855406	1244.770677	5.056960	-0.020201	2.022314
106.078304	1252.905844	5.061965	-0.020247	2.028021
106.670231	1261.025926	5.066970	-0.020362	2.033740
106.997937	1269.115535	5.071974	-0.020429	2.039394
107.350962	1277.209493	5.076979	-0.020499	2.045038
107.858807	1285.295708	5.081984	-0.020599	2.050676
108.458250	1293.390505	5.086989	-0.020715	2.056315
109.090767	1301.467008	5.091994	-0.020838	2.061928
109.755894	1309.536185	5.096998	-0.020967	2.067524
110.360644	1317.645499	5.102003	-0.021085	2.073126
110.468970	1325.778713	5.107008	-0.021110	2.078680
110.687405	1333.892006	5.112013	-0.021156	2.084217
110.943200	1342.003187	5.117018	-0.021208	2.089741
111.304159	1350.094432	5.122022	-0.021281	2.095247
111.772388	1358.181747	5.127027	-0.021373	2.100747
111.848107	1366.300964	5.132032	-0.021392	2.106215
112.459527	1374.415190	5.137037	-0.021511	2.111718
112.817661	1382.525723	5.142042	-0.021582	2.117179
113.349689	1390.560761	5.147046	-0.021686	2.122593
114.319220	1398.572309	5.152051	-0.021872	2.128019
114.490044	1406.704799	5.157056	-0.021909	2.133435
114.906439	1414.795947	5.162061	-0.021991	2.138833
115.609309	1422.839593	5.167066	-0.022127	2.144213
116.273778	1430.898574	5.172070	-0.022256	2.149586
116.756103	1439.026624	5.177075	-0.022351	2.154974
116.700185	1447.156162	5.182080	-0.022345	2.160298
117.249481	1455.214434	5.187085	-0.022453	2.165620
117.724974	1463.301541	5.192090	-0.022546	2.170940
118.034177	1471.406319	5.197094	-0.022609	2.176243
118.466225	1479.488393	5.202099	-0.022694	2.181530
119.140236	1487.532454	5.207104	-0.022825	2.186801
119.346343	1495.687353	5.212109	-0.022868	2.192089
119.695028	1503.784239	5.217114	-0.022938	2.197339
120.381436	1511.794988	5.222118	-0.023071	2.202552
121.136681	1519.852314	5.227123	-0.023217	2.207789
121.556632	1527.958710	5.232128	-0.023300	2.213014
121.924032	1536.049132	5.237133	-0.023373	2.218212
122.519350	1544.106446	5.242138	-0.023489	2.223396
122.794329	1552.196684	5.247142	-0.023545	2.228561
123.141622	1560.333990	5.252147	-0.023615	2.233751
123.417437	1568.404601	5.257152	-0.023671	2.238879
123.725279	1576.475339	5.262157	-0.023734	2.243999
124.131919	1584.550472	5.267162	-0.023814	2.249119
124.269312	1592.666860	5.272166	-0.023845	2.254229
124.643534	1600.733692	5.277171	-0.023920	2.259317
124.774494	1608.822266	5.282176	-0.023949	2.264386
125.211340	1616.888169	5.287181	-0.024035	2.269456
125.868404	1625.021276	5.292186	-0.024163	2.274575
126.114099	1633.052157	5.297190	-0.024214	2.279584
126.277925	1641.131349	5.302195	-0.024249	2.284605
126.671201	1649.169772	5.307200	-0.024327	2.289609
127.229932	1657.242044	5.312205	-0.024436	2.294637
127.546528	1665.309859	5.317210	-0.024500	2.299631
127.852557	1673.357716	5.322214	-0.024562	2.304600
128.270663	1681.454205	5.327219	-0.024645	2.309598
128.815194	1689.504221	5.332224	-0.024751	2.314567
129.186172	1697.558515	5.337229	-0.024826	2.319514
129.581918	1705.625092	5.342234	-0.024904	2.324460
129.880435	1713.700781	5.347238	-0.024965	2.329392
130.413362	1721.784066	5.352243	-0.025069	2.334338
130.701642	1729.854070	5.357248	-0.025128	2.339245
131.047494	1737.920477	5.362253	-0.025197	2.344145
131.261234	1746.022163	5.367258	-0.025242	2.349044
131.459183	1754.144615	5.372262	-0.025284	2.353945
131.985231	1762.164561	5.377267	-0.025387	2.358800
132.362556	1770.209455	5.382272	-0.025462	2.363648
132.877821	1778.256732	5.387277	-0.025563	2.368499
133.162630	1786.375438	5.392282	-0.025621	2.373363
133.380668	1794.428081	5.397286	-0.025667	2.378173
133.786457	1802.480685	5.402291	-0.025747	2.382989
134.144768	1810.557532	5.407296	-0.025819	2.387805
134.718744	1818.615756	5.412301	-0.025931	2.392617
135.039680	1826.686003	5.417306	-0.025995	2.397407
135.181170	1834.745084	5.422310	-0.026027	2.402166
135.704929	1842.786899	5.427315	-0.026129	2.406936
135.698902	1850.889085	5.432320	-0.026133	2.411690
136.106726	1858.951799	5.437325	-0.026214	2.416444
136.463858	1867.002367	5.442330	-0.026286	2.421177
136.714090	1875.052547	5.447334	-0.026337	2.425893
136.986360	1883.164760	5.452339	-0.026393	2.430637
137.053139	1891.308026	5.457344	-0.026410	2.435374
137.655780	1899.290182	5.462349	-0.026528	2.440050
137.970852	1907.314271	5.467354	-0.026591	2.444718
138.387523	1915.345163	5.472358	-0.026674	2.449390
138.853618	1923.424740	5.477363	-0.026766	2.454084
139.266703	1931.458628	5.482368	-0.026847	2.458739
139.377963	1939.535790	5.487373	-0.026873	2.463387
139.648869	1947.618615	5.492378	-0.026929	2.468042
139.964231	1955.675864	5.497382	-0.026992	2.472676
140.377203	1963.730808	5.502387	-0.027074	2.477308
140.753779	1971.764997	5.507392	-0.027149	2.481916
141.178172	1979.813101	5.512397	-0.027233	2.486527
141.190345	1987.925171	5.517402	-0.027241	2.491136
141.413005	1995.985909	5.522406	-0.027287	2.495722
141.979033	2004.020570	5.527411	-0.027397	2.500311
142.472650	2012.025208	5.532416	-0.027494	2.504868
142.499429	2020.140903	5.537421	-0.027504	2.509446
142.953905	2028.239197	5.542426	-0.027594	2.514036
143.341231	2036.244678	5.547430	-0.027671	2.518562
143.578444	2044.298266	5.552435	-0.027720	2.523095
143.902434	2052.341707	5.557440	-0.027786	2.527620
144.110612	2060.423246	5.562445	-0.027829	2.532151
144.427615	2068.498223	5.567450	-0.027893	2.536677
144.667660	2076.535898	5.572454	-0.027943	2.541169
145.026071	2084.580479	5.577459	-0.028015	2.545665
145.489194	2092.621984	5.582464	-0.028106	2.550159
145.611249	2100.713901	5.587469	-0.028134	2.554649
146.060005	2108.743427	5.592474	-0.028222	2.559119
146.395396	2116.755750	5.597478	-0.028290	2.563564
146.793250	2124.833578	5.602483	-0.028369	2.568041
146.933791	2132.913026	5.607488	-0.028400	2.572494
147.384495	2140.962400	5.612493	-0.028489	2.576944
147.835363	2149.002573	5.617498	-0.028578	2.581381
147.934706	2157.056140	5.622502	-0.028601	2.585794
148.447272	2165.136981	5.627507	-0.028702	2.590242
148.990826	2173.339061	5.632512	-0.028808	2.594751
149.079291	2181.341885	5.637517	-0.028829	2.599112
149.339438	2189.358657	5.642522	-0.028883	2.603485
149.828215	2197.338714	5.647526	-0.028979	2.607847
150.158465	2205.404937	5.652531	-0.029045	2.612237
150.417306	2213.439467	5.657536	-0.029098	2.616598
150.801052	2221.457319	5.662541	-0.029175	2.620950
151.453897	2229.489659	5.667546	-0.029301	2.625321
151.935203	2237.489589	5.672550	-0.029396	2.629656
152.255801	2245.607790	5.677555	-0.029461	2.634037
152.507892	2253.658090	5.682560	-0.029513	2.638369
152.633343	2261.715165	5.687565	-0.029541	2.642689
152.874510	2269.772765	5.692570	-0.029591	2.647011
153.184839	2277.812364	5.697574	-0.029654	2.651320
153.503869	2285.895848	5.702579	-0.029718	2.655645
153.611441	2293.937449	5.707584	-0.029743	2.659928
154.026371	2301.956947	5.712589	-0.029825	2.664212
154.199549	2310.030834	5.717594	-0.029863	2.668502
154.275967	2318.126045	5.722598	-0.029882	2.672791
154.550682	2326.164700	5.727603	-0.029938	2.677055
155.090755	2334.163451	5.732608	-0.030043	2.681309
155.275415	2342.201613	5.737613	-0.030083	2.685553
155.803554	2350.215872	5.742618	-0.030186	2.689800
156.306405	2358.261638	5.747622	-0.030285	2.694056
156.344473	2366.363271	5.752627	-0.030297	2.698304
156.534190	2374.408721	5.757632	-0.030337	2.702526
156.846264	2382.450988	5.762637	-0.030400	2.706747
157.225994	2390.508673	5.767642	-0.030476	2.710974
157.314683	2398.567184	5.772646	-0.030497	2.715177
157.887568	2406.581615	5.777651	-0.030609	2.719380
158.620344	2414.565046	5.782656	-0.030750	2.723570
159.363505	2422.575636	5.787661	-0.030894	2.727769
159.856740	2430.651643	5.792666	-0.030991	2.731979
160.054275	2438.750088	5.797670	-0.031032	2.736176
160.424496	2446.800068	5.802675	-0.031106	2.740352
160.467780	2454.848446	5.807680	-0.031119	2.744502
160.895218	2462.872189	5.812685	-0.031204	2.748655
161.396592	2470.995715	5.817690	-0.031302	2.752858
161.723164	2479.023973	5.822694	-0.031368	2.756995
162.187532	2487.031823	5.827699	-0.031460	2.761123
162.729765	2495.012245	5.832704	-0.031565	2.765236
162.927003	2503.083193	5.837709	-0.031607	2.769369
163.239007	2511.179256	5.842714	-0.031670	2.773514
163.155404	2519.230045	5.847718	-0.031660	2.777607
163.462795	2527.252040	5.852723	-0.031722	2.781703
163.936059	2535.266749	5.857728	-0.031815	2.785798
164.170270	2543.320661	5.862733	-0.031864	2.789893
164.637744	2551.399026	5.867738	-0.031956	2.794008
164.722341	2559.421951	5.872742	-0.031976	2.798067
165.010298	2567.479533	5.877747	-0.032035	2.802149
165.207434	2575.516095	5.882752	-0.032077	2.806209
165.490444	2583.553906	5.887757	-0.032134	2.810269
166.218878	2591.580304	5.892762	-0.032275	2.814343
166.490233	2599.613259	5.897766	-0.032330	2.818388
166.849275	2607.642256	5.902771	-0.032402	2.822430
167.086687	2615.702496	5.907776	-0.032452	2.826475
167.565303	2623.733755	5.912781	-0.032546	2.830513
167.746395	2631.867037	5.917786	-0.032584	2.834580
167.857813	2639.868840	5.922790	-0.032610	2.838571
168.132553	2647.892954	5.927795	-0.032666	2.842577
168.634266	2655.908478	5.932800	-0.032765	2.846585
168.796262	2663.973398	5.937805	-0.032800	2.850594
169.035792	2672.049839	5.942810	-0.032849	2.854606
169.391561	2680.040646	5.947814	-0.032921	2.858577
169.822308	2688.058367	5.952819	-0.033006	2.862560
170.091836	2696.119554	5.957824	-0.033061	2.866550
170.471735	2704.155002	5.962829	-0.033137	2.870528
170.985091	2712.212278	5.967834	-0.033237	2.874518
171.106860	2720.243378	5.972838	-0.033265	2.878469
171.417044	2728.290677	5.977843	-0.033328	2.882432
171.626632	2736.332363	5.982848	-0.033372	2.886381
171.751033	2744.363992	5.987853	-0.033400	2.890315
172.001655	2752.459798	5.992858	-0.033451	2.894283
172.253998	2760.464168	5.997862	-0.033503	2.898200
172.673300	2768.499528	6.002867	-0.033586	2.902136
172.897996	2776.543754	6.007872	-0.033633	2.906060
173.089609	2784.586547	6.012877	-0.033674	2.909977
173.577345	2792.706894	6.017882	-0.033770	2.913941
173.868782	2800.705983	6.022886	-0.033829	2.917831
174.198640	2808.708468	6.027891	-0.033895	2.921720
174.394483	2816.736464	6.032896	-0.033937	2.925608
174.798575	2824.742140	6.037901	-0.034017	2.929492
175.365104	2832.813572	6.042906	-0.034127	2.933410
175.395372	2840.853195	6.047910	-0.034138	2.937280
175.620584	2848.910865	6.052915	-0.034185	2.941163
175.942671	2856.899145	6.057920	-0.034250	2.945013
176.142723	2864.933434	6.062925	-0.034292	2.948874
176.623179	2873.004193	6.067930	-0.034387	2.952761
176.735871	2881.046443	6.072934	-0.034413	2.956611
177.040786	2889.075923	6.077939	-0.034474	2.960460
177.319210	2897.091344	6.082944	-0.034531	2.964295
177.796989	2905.114939	6.087949	-0.034625	2.968139
178.013057	2913.191680	6.092954	-0.034670	2.971991
178.274717	2921.228752	6.097958	-0.034724	2.975820
178.781530	2929.235670	6.102963	-0.034823	2.979643
179.030510	2937.276652	6.107968	-0.034875	2.983464
179.100088	2945.331303	6.112973	-0.034893	2.987278
179.429469	2953.383928	6.117978	-0.034959	2.991099
179.768303	2961.426826	6.122982	-0.035027	2.994910
180.071958	2969.449401	6.127987	-0.035089	2.998706
180.131438	2977.488826	6.132992	-0.035105	3.002492
180.390285	2985.517434	6.137997	-0.035158	3.006278
180.731837	2993.543616	6.143002	-0.035226	3.010063
180.738015	3001.613285	6.148006	-0.035233	3.013846
181.013053	3009.638252	6.153011	-0.035289	3.017618
181.297668	3017.666393	6.158016	-0.035347	3.021386
181.475104	3025.669080	6.163021	-0.035385	3.025132
181.789494	3033.734485	6.168026	-0.035448	3.028910
181.932694	3041.791723	6.173030	-0.035480	3.032671
182.342988	3049.840722	6.178035	-0.035561	3.036436
182.337320	3057.855636	6.183040	-0.035565	3.040160
182.696629	3065.875623	6.188045	-0.035637	3.043900
182.981145	3073.932252	6.193050	-0.035695	3.047649
183.149217	3081.960348	6.198054	-0.035731	3.051374
183.370666	3090.011775	6.203059	-0.035777	3.055108
183.794981	3098.014480	6.208064	-0.035861	3.058824
184.080330	3106.035282	6.213069	-0.035920	3.062538
184.545071	3114.082212	6.218074	-0.036011	3.066267
184.927400	3122.089894	6.223078	-0.036087	3.069970
185.274630	3130.222484	6.228083	-0.036157	3.073725
185.320306	3138.276087	6.233088	-0.036170	3.077424
185.488056	3146.269117	6.238093	-0.036207	3.081097
186.228683	3154.187854	6.243098	-0.036349	3.084757
186.267194	3162.256307	6.248102	-0.036362	3.088450
186.552450	3170.325966	6.253107	-0.036420	3.092150
186.898830	3178.368485	6.258112	-0.036489	3.095836
187.168798	3186.359909	6.263117	-0.036544	3.099490
187.254556	3194.425355	6.268122	-0.036565	3.103166
187.425606	3202.441039	6.273126	-0.036602	3.106818
187.715130	3210.496373	6.278131	-0.036661	3.110490
188.175107	3218.527170	6.283136	-0.036752	3.114153
188.476016	3226.529713	6.288141	-0.036813	3.117793
188.710706	3234.596659	6.293146	-0.036861	3.121454
188.719298	3242.609221	6.298150	-0.036868	3.125076
188.936602	3250.665799	6.303155	-0.036913	3.128723
189.471390	3258.696400	6.308160	-0.037018	3.132368
189.404276	3266.759171	6.313165	-0.037010	3.135997
189.596587	3274.774503	6.318170	-0.037051	3.139612
190.008754	3282.760225	6.323174	-0.037133	3.143219
190.170883	3290.820877	6.328179	-0.037168	3.146844
190.189277	3298.884756	6.333184	-0.037177	3.150460
190.609431	3306.904778	6.338189	-0.037260	3.154070
190.958750	3314.934816	6.343194	-0.037330	3.157677
191.006622	3322.952466	6.348198	-0.037344	3.161262
191.360837	3330.938345	6.353203	-0.037415	3.164841
191.875605	3338.966264	6.358208	-0.037515	3.168442
191.929949	3347.036114	6.363213	-0.037530	3.172037
192.351860	3355.093077	6.368218	-0.037614	3.175639
192.779316	3363.078011	6.373222	-0.037699	3.179205
193.127801	3371.114199	6.378227	-0.037768	3.182786
193.194557	3379.166870	6.383232	-0.037786	3.186358
193.577151	3387.177263	6.388237	-0.037862	3.189921
193.891176	3395.242196	6.393242	-0.037926	3.193501
193.831740	3403.300980	6.398246	-0.037919	3.197058
194.181381	3411.313575	6.403251	-0.037990	3.200608
194.481663	3419.304491	6.408256	-0.038050	3.204143
194.745395	3427.344736	6.413261	-0.038104	3.207694
194.982402	3435.415728	6.418266	-0.038154	3.211254
195.144613	3443.438140	6.423270	-0.038189	3.214785
195.522325	3451.454891	6.428275	-0.038264	3.218318
195.620931	3459.513246	6.433280	-0.038287	3.221854
195.957511	3467.492595	6.438285	-0.038355	3.225362
196.539445	3475.526438	6.443290	-0.038468	3.228899
196.768585	3483.599421	6.448294	-0.038516	3.232436
196.834873	3491.688643	6.453299	-0.038533	3.235969
197.317215	3499.628449	6.458304	-0.038628	3.239449
197.480483	3507.633141	6.463309	-0.038663	3.242942
197.790178	3515.689022	6.468314	-0.038726	3.246458
198.108669	3523.686846	6.473318	-0.038790	3.249946
198.447657	3531.745513	6.478323	-0.038859	3.253457
198.577577	3539.798405	6.483328	-0.038888	3.256954
198.523647	3547.822063	6.488333	-0.038883	3.260427
198.969638	3555.829458	6.493338	-0.038971	3.263909
199.321879	3563.844067	6.498342	-0.039041	3.267387
199.506290	3571.893535	6.503347	-0.039080	3.270869
200.067343	3579.927582	6.508352	-0.039190	3.274355
200.325702	3587.938469	6.513357	-0.039243	3.277817
200.616948	3596.007242	6.518362	-0.039302	3.281300
201.018561	3603.957779	6.523366	-0.039382	3.284733
201.456291	3612.001597	6.528371	-0.039468	3.288204
201.537624	3620.088366	6.533376	-0.039489	3.291676
201.833288	3628.111275	6.538381	-0.039549	3.295126
202.342296	3636.134584	6.543386	-0.039648	3.298579
202.325753	3644.168945	6.548390	-0.039650	3.302014
202.559789	3652.175439	6.553395	-0.039699	3.305443
202.877142	3660.195400	6.558400	-0.039763	3.308877
203.118191	3668.264332	6.563405	-0.039813	3.312326
203.288627	3676.328244	6.568410	-0.039849	3.315766
203.481617	3684.310508	6.573414	-0.039890	3.319169
203.910280	3692.306011	6.578419	-0.039975	3.322582
204.179714	3700.341616	6.583424	-0.040030	3.326003
204.407762	3708.352433	6.588429	-0.040078	3.329409
204.863470	3716.409143	6.593434	-0.040168	3.332839
204.987277	3724.456880	6.598438	-0.040196	3.336249
204.979848	3732.473376	6.603443	-0.040199	3.339637
205.189213	3740.526493	6.608448	-0.040243	3.343046
205.240748	3748.541664	6.613453	-0.040258	3.346429
205.413723	3756.606340	6.618458	-0.040295	3.349835
205.709766	3764.636775	6.623462	-0.040355	3.353226
206.144101	3772.662080	6.628467	-0.040441	3.356617
206.354181	3780.664453	6.633472	-0.040485	3.359987
206.691248	3788.665556	6.638477	-0.040553	3.363358
207.076188	3796.724386	6.643482	-0.040629	3.366751
207.345011	3804.709739	6.648486	-0.040684	3.370105
207.831672	3812.774184	6.653491	-0.040780	3.373497
208.004016	3820.820666	6.658496	-0.040817	3.376867
208.239745	3828.819036	6.663501	-0.040866	3.380216
208.411882	3836.872016	6.668506	-0.040903	3.383582
208.474859	3844.877871	6.673510	-0.040920	3.386921
208.690375	3852.921569	6.678515	-0.040965	3.390278
208.798149	3861.070262	6.683520	-0.040990	3.393671
209.151247	3869.057012	6.688525	-0.041060	3.397002
209.319155	3877.012344	6.693530	-0.041097	3.400310
209.432595	3884.998132	6.698534	-0.041123	3.403626
209.740805	3893.032839	6.703539	-0.041185	3.406966
210.163430	3901.017024	6.708544	-0.041269	3.410285
210.315050	3909.097375	6.713549	-0.041302	3.413632
210.649909	3917.134287	6.718554	-0.041369	3.416963
210.831282	3925.104831	6.723558	-0.041408	3.420259
211.226251	3933.123907	6.728563	-0.041487	3.423578
211.298982	3941.172111	6.733568	-0.041505	3.426896
211.427996	3949.206844	6.738573	-0.041534	3.430206
211.766028	3957.291588	6.743578	-0.041602	3.433541
211.908792	3965.290000	6.748582	-0.041634	3.436831
212.026284	3973.315713	6.753587	-0.041660	3.440128
212.137296	3981.351236	6.758592	-0.041686	3.443425
212.497989	3989.361341	6.763597	-0.041758	3.446717
212.779739	3997.384892	6.768602	-0.041816	3.450009
212.788596	4005.411480	6.773606	-0.041822	3.453290
213.491071	4013.451931	6.778611	-0.041958	3.456596
213.671293	4021.477966	6.783616	-0.041997	3.459876
214.121246	4029.476341	6.788621	-0.042085	3.463151
214.326291	4037.554972	6.793626	-0.042128	3.466447
214.549888	4045.546238	6.798630	-0.042175	3.469704
214.792144	4053.625883	6.803635	-0.042225	3.472996
214.990956	4061.655205	6.808640	-0.042267	3.476262
215.196072	4069.612364	6.813645	-0.042310	3.479496
215.551188	4077.651533	6.818650	-0.042381	3.482765
215.554848	4085.669734	6.823654	-0.042387	3.486011
215.892255	4093.678514	6.828659	-0.042455	3.489261
216.208037	4101.698160	6.833664	-0.042519	3.492512
216.257050	4109.764039	6.838669	-0.042533	3.495770
216.515263	4117.775500	6.843674	-0.042586	3.499009
216.623305	4125.795317	6.848678	-0.042611	3.502244
216.672343	4133.820192	6.853683	-0.042625	3.505476
216.959495	4141.849641	6.858688	-0.042683	3.508715
217.127386	4149.899723	6.863693	-0.042720	3.511955
217.845894	4157.906448	6.868698	-0.042858	3.515191
218.020157	4165.894861	6.873702	-0.042896	3.518401
218.053977	4173.948939	6.878707	-0.042907	3.521629
218.677600	4181.931901	6.883712	-0.043028	3.524844
218.740030	4189.966696	6.888717	-0.043045	3.528060
219.059457	4198.052667	6.893722	-0.043109	3.531301
218.977146	4206.078833	6.898726	-0.043099	3.534503
219.312344	4214.119881	6.903731	-0.043166	3.537720
219.533137	4222.156647	6.908736	-0.043212	3.540930
219.634021	4230.132939	6.913741	-0.043236	3.544109
219.944287	4238.194196	6.918746	-0.043299	3.547325
219.988546	4246.207345	6.923750	-0.043312	3.550511
220.338230	4254.323737	6.928755	-0.043382	3.553744
220.701865	4262.346661	6.933760	-0.043455	3.556937
220.823683	4270.296388	6.938765	-0.043482	3.560092
221.321318	4278.301951	6.943770	-0.043580	3.563277
221.493953	4286.332557	6.948774	-0.043617	3.566459
221.743466	4294.311036	6.953779	-0.043669	3.569620
221.908649	4302.378814	6.958784	-0.043704	3.572811
222.103478	4310.397100	6.963789	-0.043746	3.575980
222.350375	4318.389482	6.968794	-0.043797	3.579138
222.499068	4326.419182	6.973798	-0.043829	3.582305
222.636561	4334.433858	6.978803	-0.043860	3.585463
222.984928	4342.462650	6.983808	-0.043930	3.588630
222.962514	4350.512738	6.988813	-0.043930	3.591791
223.253810	4358.540968	6.993818	-0.043990	3.594951
223.228023	4366.555352	6.998822	-0.043990	3.598092
223.657963	4374.575202	7.003827	-0.044075	3.601247
224.023080	4382.563826	7.008832	-0.044148	3.604384
224.208082	4390.586780	7.013837	-0.044187	3.607527
224.501477	4398.636300	7.018842	-0.044247	3.610680
224.742673	4406.655893	7.023846	-0.044297	3.613818
224.864666	4414.682980	7.028851	-0.044324	3.616953
225.291358	4422.698842	7.033856	-0.044409	3.620088
225.558505	4430.706587	7.038861	-0.044463	3.623214
225.740004	4438.783567	7.043866	-0.044502	3.626361
225.999355	4446.795525	7.048870	-0.044556	3.629482
226.298469	4454.843098	7.053875	-0.044616	3.632616
226.534880	4462.897286	7.058880	-0.044665	3.635748
226.711708	4470.856318	7.063885	-0.044703	3.638838
226.969845	4478.908503	7.068890	-0.044756	3.641964
227.166818	4486.879138	7.073894	-0.044798	3.645054
227.300151	4494.940960	7.078899	-0.044828	3.648175
227.568200	4502.968194	7.083904	-0.044882	3.651284
227.896752	4510.973184	7.088909	-0.044949	3.654383
228.164007	4519.024925	7.093914	-0.045003	3.657495
228.369140	4527.022221	7.098918	-0.045047	3.660583
228.518305	4535.048000	7.103923	-0.045079	3.663677
229.094960	4543.089130	7.108928	-0.045192	3.666786
229.070963	4551.082703	7.113933	-0.045192	3.669858
229.388270	4559.175545	7.118938	-0.045256	3.672974
229.673032	4567.195382	7.123942	-0.045314	3.676059
229.777779	4575.172188	7.128947	-0.045339	3.679120
230.218813	4583.214850	7.133952	-0.045426	3.682212
230.417289	4591.186726	7.138957	-0.045468	3.685269
230.746283	4599.248966	7.143962	-0.045534	3.688361
230.773320	4607.294712	7.148966	-0.045544	3.691436
230.990076	4615.313447	7.153971	-0.045589	3.694503
231.212442	4623.345948	7.158976	-0.045636	3.697573
231.152100	4631.334055	7.163981	-0.045629	3.700616
231.494023	4639.354994	7.168986	-0.045698	3.703679
231.819443	4647.390370	7.173990	-0.045764	3.706745
232.019564	4655.393841	7.178995	-0.045806	3.709793
232.281933	4663.516713	7.184000	-0.045860	3.712885
232.381104	4671.522043	7.189005	-0.045883	3.715927
232.642714	4679.540028	7.194010	-0.045937	3.718974
232.780948	4687.485244	7.199014	-0.045967	3.721988
232.991196	4695.469491	7.204019	-0.046011	3.725017
233.357015	4703.534643	7.209024	-0.046085	3.728077
233.381079	4711.546464	7.214029	-0.046094	3.731106
233.732717	4719.591241	7.219034	-0.046165	3.734153
233.724921	4727.611607	7.224038	-0.046168	3.737180
233.972836	4735.605024	7.229043	-0.046219	3.740200
234.128040	4743.664701	7.234048	-0.046253	3.743241
234.355385	4751.636909	7.239053	-0.046300	3.746247
234.623257	4759.677035	7.244058	-0.046355	3.749278
234.650614	4767.751174	7.249062	-0.046365	3.752314
234.885268	4775.753356	7.254067	-0.046414	3.755325
235.014586	4783.791034	7.259072	-0.046443	3.758344
235.038969	4791.824195	7.264077	-0.046452	3.761357
235.484302	4799.761338	7.269082	-0.046540	3.764341
235.634054	4807.851505	7.274086	-0.046573	3.767373
235.653510	4815.877708	7.279091	-0.046582	3.770376
235.999132	4823.919782	7.284096	-0.046651	3.773389
236.107490	4831.927597	7.289101	-0.046676	3.776382
236.418304	4839.907018	7.294106	-0.046739	3.779367
236.750930	4847.964451	7.299110	-0.046806	3.782379
236.792953	4855.950296	7.304115	-0.046819	3.785355
236.957267	4864.034148	7.309120	-0.046854	3.788368
237.196338	4872.039463	7.314125	-0.046904	3.791351
237.407146	4880.103286	7.319130	-0.046948	3.794353
237.640734	4888.103289	7.324134	-0.046997	3.797329
237.783812	4896.049362	7.329139	-0.047028	3.800281
237.947568	4904.098171	7.334144	-0.047064	3.803269
238.453352	4912.084481	7.339149	-0.047163	3.806239
238.677801	4920.120661	7.344154	-0.047210	3.809219
238.581180	4928.174303	7.349158	-0.047197	3.812196
239.037078	4936.192056	7.354163	-0.047286	3.815169
239.422909	4944.190717	7.359168	-0.047363	3.818132
239.462793	4952.196209	7.364173	-0.047376	3.821087
240.018059	4960.191914	7.369178	-0.047484	3.824047
240.280561	4968.224358	7.374182	-0.047538	3.827013
240.650647	4976.223094	7.379187	-0.047612	3.829966
240.803224	4984.322014	7.384192	-0.047645	3.832948
241.064285	4992.339618	7.389197	-0.047699	3.835901
241.255162	5000.364076	7.394202	-0.047739	3.838853
241.298112	5008.429486	7.399206	-0.047752	3.841814
241.579213	5016.320055	7.404211	-0.047809	3.844714
241.887472	5024.423131	7.409216	-0.047872	3.847689
241.895401	5032.412005	7.414221	-0.047878	3.850615
242.178037	5040.470271	7.419226	-0.047936	3.853569
242.268285	5048.502760	7.424230	-0.047958	3.856508
242.631295	5056.487095	7.429235	-0.048030	3.859433
242.781309	5064.539798	7.434240	-0.048063	3.862375
242.984913	5072.521302	7.439245	-0.048106	3.865291
243.320180	5080.595152	7.444250	-0.048173	3.868241
243.445046	5088.617272	7.449254	-0.048202	3.871165
243.756021	5096.849994	7.454259	-0.048265	3.874167
244.102047	5104.806533	7.459264	-0.048334	3.877068
244.061391	5112.739220	7.464269	-0.048331	3.879950
244.488400	5120.731925	7.469274	-0.048416	3.882860
244.509930	5128.734334	7.474278	-0.048425	3.885764
244.965641	5136.715402	7.479283	-0.048514	3.888667
245.012930	5144.783705	7.484288	-0.048528	3.891591
245.171971	5152.779753	7.489293	-0.048563	3.894489
245.360634	5160.815673	7.494298	-0.048603	3.897400
245.582235	5168.797216	7.499302	-0.048649	3.900289
245.719941	5176.818545	7.504307	-0.048680	3.903189
245.894224	5184.838816	7.509312	-0.048717	3.906087
245.999540	5192.840114	7.514317	-0.048742	3.908975
246.166116	5200.943881	7.519322	-0.048778	3.911899
246.485647	5208.925399	7.524326	-0.048842	3.914779
246.684666	5216.921701	7.529331	-0.048884	3.917660
247.069769	5224.918849	7.534336	-0.048961	3.920543
247.018255	5232.914650	7.539341	-0.048956	3.923415
247.542445	5240.948959	7.544346	-0.049059	3.926310
247.630009	5248.992255	7.549350	-0.049080	3.929197
247.836157	5257.010306	7.554355	-0.049124	3.932076
248.311968	5265.064445	7.559360	-0.049217	3.934970
248.356226	5273.040635	7.564365	-0.049230	3.937826
248.510197	5281.070459	7.569370	-0.049264	3.940702
248.880866	5289.059704	7.574374	-0.049338	3.943564
249.136805	5297.073673	7.579379	-0.049391	3.946432
249.476707	5305.133222	7.584384	-0.049459	3.949314
249.469890	5313.180697	7.589389	-0.049463	3.952185
249.842140	5321.212109	7.594394	-0.049537	3.955054
250.181648	5329.204628	7.599398	-0.049605	3.957906
250.101588	5337.175019	7.604403	-0.049595	3.960742
250.351806	5345.229203	7.609408	-0.049647	3.963611
250.576246	5353.207963	7.614413	-0.049693	3.966450
250.815201	5361.261324	7.619418	-0.049743	3.969314
250.983684	5369.314270	7.624422	-0.049779	3.972175
251.129475	5377.331017	7.629427	-0.049811	3.975020
251.193508	5385.375929	7.634432	-0.049828	3.977872
251.294822	5393.360520	7.639437	-0.049852	3.980701
251.558649	5401.366211	7.644442	-0.049906	3.983539
251.638485	5409.409234	7.649446	-0.049926	3.986384
251.846048	5417.382314	7.654451	-0.049970	3.989205
252.126178	5425.423242	7.659456	-0.050027	3.992049
252.183818	5433.482884	7.664461	-0.050042	3.994893
252.433017	5441.528929	7.669466	-0.050094	3.997734
252.706938	5449.524730	7.674470	-0.050150	4.000556
253.015466	5457.506105	7.679475	-0.050212	4.003371
253.179128	5465.559235	7.684480	-0.050248	4.006207
253.097420	5473.574084	7.689485	-0.050237	4.009024
253.371236	5481.637326	7.694490	-0.050293	4.011861
253.548906	5489.677762	7.699494	-0.050331	4.014687
253.745415	5497.665250	7.704499	-0.050373	4.017492
253.951477	5505.692729	7.709504	-0.050416	4.020310
254.249677	5513.668404	7.714509	-0.050477	4.023109
254.503527	5521.702550	7.719514	-0.050529	4.025926
254.568201	5529.736383	7.724518	-0.050546	4.028737
254.630548	5537.753630	7.729523	-0.050563	4.031541
255.048127	5545.918508	7.734528	-0.050645	4.034400
254.937880	5553.860642	7.739533	-0.050630	4.037171
255.201269	5561.811922	7.744538	-0.050684	4.039949
255.476527	5569.807702	7.749542	-0.050740	4.042741
255.491926	5577.810272	7.754547	-0.050748	4.045529
255.703616	5585.854058	7.759552	-0.050792	4.048332
256.133393	5593.849484	7.764557	-0.050877	4.051120
256.249427	5601.917602	7.769562	-0.050904	4.053927
256.389569	5609.946318	7.774566	-0.050935	4.056718
256.763394	5617.887306	7.779571	-0.051009	4.059481
256.945696	5625.951569	7.784576	-0.051048	4.062281
257.101041	5633.888367	7.789581	-0.051082	4.065035
257.415818	5641.933187	7.794586	-0.051146	4.067827
257.751135	5649.940442	7.799590	-0.051213	4.070604
257.798423	5657.993831	7.804595	-0.051227	4.073391
258.115051	5666.063614	7.809600	-0.051291	4.076185
258.314633	5674.019019	7.814605	-0.051333	4.078937
258.382087	5682.089162	7.819610	-0.051351	4.081724
258.391615	5690.047674	7.824614	-0.051357	4.084470
258.775861	5698.080110	7.829619	-0.051434	4.087245
258.930103	5706.070092	7.834624	-0.051467	4.090000
258.973633	5714.104318	7.839629	-0.051480	4.092767
259.441868	5722.167449	7.844634	-0.051573	4.095548
259.499999	5730.206696	7.849638	-0.051588	4.098313
259.397684	5738.195770	7.854643	-0.051574	4.101057
259.643272	5746.217777	7.859648	-0.051625	4.103815
259.846959	5754.197741	7.864653	-0.051668	4.106556
260.164112	5762.259882	7.869658	-0.051732	4.109325
260.164092	5770.304005	7.874662	-0.051737	4.112082
260.391059	5778.346852	7.879667	-0.051784	4.114839
260.820399	5786.392215	7.884672	-0.051869	4.117598
260.914751	5794.314954	7.889677	-0.051892	4.120309
260.890612	5802.378907	7.894682	-0.051892	4.123065
260.993908	5810.351225	7.899686	-0.051916	4.125789
261.343639	5818.379342	7.904691	-0.051986	4.128534
261.475537	5826.428184	7.909696	-0.052016	4.131281
261.630704	5834.483438	7.914701	-0.052050	4.134028
262.097723	5842.534759	7.919706	-0.052142	4.136777
262.206743	5850.473225	7.924710	-0.052167	4.139480
262.443983	5858.470215	7.929715	-0.052216	4.142204
262.694946	5866.506078	7.934720	-0.052268	4.144938
262.699031	5874.537645	7.939725	-0.052274	4.147667
262.778942	5882.589339	7.944730	-0.052293	4.150402
263.195063	5890.601566	7.949734	-0.052376	4.153125
263.166993	5898.613390	7.954739	-0.052376	4.155841
263.397187	5906.647386	7.959744	-0.052423	4.158566
263.439969	5914.625827	7.964749	-0.052436	4.161268
263.851038	5922.614506	7.969754	-0.052518	4.163976
263.746368	5930.692467	7.974758	-0.052503	4.166707
263.954287	5938.645987	7.979763	-0.052547	4.169397
264.340031	5946.706993	7.984768	-0.052624	4.172124
264.170197	5954.757635	7.989773	-0.052597	4.174839
264.454242	5962.742928	7.994778	-0.052655	4.177535
264.839128	5970.749654	7.999782	-0.052732	4.180238
264.893751	5978.780837	8.004787	-0.052747	4.182944
265.040203	5986.780875	8.009792	-0.052779	4.185639
265.153106	5994.800213	8.014797	-0.052805	4.188338
265.568266	6002.855046	8.019802	-0.052887	4.191050
265.800624	6010.944330	8.024806	-0.052936	4.193770
266.016318	6018.959502	8.029811	-0.052981	4.196464
266.281070	6026.888092	8.034816	-0.053035	4.199127
266.447547	6034.915240	8.039821	-0.053071	4.201820
266.686170	6042.883866	8.044826	-0.053120	4.204493
266.853335	6050.924216	8.049830	-0.053156	4.207187
266.764840	6058.894580	8.054835	-0.053145	4.209854
266.764055	6066.962540	8.059840	-0.053150	4.212552
266.932377	6074.979172	8.064845	-0.053186	4.215233
267.243863	6082.983592	8.069850	-0.053249	4.217910
267.421925	6091.024346	8.074854	-0.053287	4.220596
267.447358	6099.012109	8.079859	-0.053297	4.223261
267.994612	6107.051378	8.084864	-0.053404	4.225946
268.053788	6115.046543	8.089869	-0.053420	4.228611
268.170287	6123.078880	8.094874	-0.053446	4.231286
268.364428	6131.166671	8.099878	-0.053487	4.233979
268.696889	6139.158997	8.104883	-0.053554	4.236640
268.975693	6147.092236	8.109888	-0.053611	4.239279
268.986016	6155.130291	8.114893	-0.053618	4.241949
269.079622	6163.161671	8.119898	-0.053640	4.244615
269.243185	6171.205608	8.124902	-0.053676	4.247285
269.454038	6179.166693	8.129907	-0.053720	4.249926
269.780926	6187.254067	8.134912	-0.053786	4.252608
269.921938	6195.244229	8.139917	-0.053817	4.255254
270.057312	6203.302824	8.144922	-0.053847	4.257922
270.174927	6211.300899	8.149926	-0.053874	4.260567
270.332831	6219.292525	8.154931	-0.053909	4.263210
270.419832	6227.346858	8.159936	-0.053930	4.265870
270.542078	6235.354233	8.164941	-0.053957	4.268514
270.946371	6243.392391	8.169946	-0.054038	4.271169
271.024628	6251.452714	8.174950	-0.054057	4.273826
271.132916	6259.428202	8.179955	-0.054082	4.276454
271.585924	6267.440620	8.184960	-0.054172	4.279096
271.782640	6275.443803	8.189965	-0.054213	4.281730
271.897222	6283.447421	8.194970	-0.054240	4.284363
272.205771	6291.497738	8.199974	-0.054302	4.287011
272.185870	6299.450992	8.204979	-0.054303	4.289622
272.436197	6307.533762	8.209984	-0.054355	4.292277
272.750821	6315.577227	8.214989	-0.054418	4.294917
272.925065	6323.578679	8.219994	-0.054456	4.297541
272.979698	6331.599411	8.224998	-0.054471	4.300169
273.264735	6339.555675	8.230003	-0.054529	4.302776
273.505480	6347.606703	8.235008	-0.054579	4.305412
273.313553	6355.659538	8.240013	-0.054548	4.308043
273.529669	6363.659002	8.245018	-0.054593	4.310659
273.695156	6371.677017	8.250022	-0.054629	4.313279
273.818596	6379.687546	8.255027	-0.054657	4.315894
274.154061	6387.697228	8.260032	-0.054724	4.318509
274.162356	6395.708718	8.265037	-0.054731	4.321121
274.313099	6403.710389	8.270042	-0.054764	4.323728
274.442011	6411.736624	8.275046	-0.054793	4.326342
274.542634	6419.716563	8.280051	-0.054817	4.328940
274.941673	6427.788988	8.285056	-0.054896	4.331567
275.202531	6435.782005	8.290061	-0.054949	4.334167
275.529673	6443.841983	8.295066	-0.055015	4.336787
275.790600	6451.800611	8.300070	-0.055069	4.339372
276.138958	6459.839287	8.305075	-0.055139	4.341982
276.194968	6467.840834	8.310080	-0.055154	4.344576
276.013452	6475.868452	8.315085	-0.055125	4.347176
276.246063	6483.877929	8.320090	-0.055173	4.349771
276.837717	6491.956479	8.325094	-0.055289	4.352389
276.883382	6500.009495	8.330099	-0.055302	4.354994
277.183254	6508.023694	8.335104	-0.055363	4.357586
277.150124	6515.916846	8.340109	-0.055362	4.360135
277.523402	6523.991517	8.345114	-0.055436	4.362744
277.954994	6531.932614	8.350118	-0.055521	4.365309
278.024749	6539.966774	8.355123	-0.055539	4.367900
278.304984	6548.029895	8.360128	-0.055597	4.370500
278.392594	6556.067574	8.365133	-0.055618	4.373089
278.852583	6564.091577	8.370138	-0.055709	4.375674
279.219133	6572.082409	8.375142	-0.055782	4.378247
279.401741	6580.066829	8.380147	-0.055821	4.380815
279.637961	6588.100745	8.385152	-0.055870	4.383397
279.730113	6596.098268	8.390157	-0.055892	4.385966
279.835982	6604.113907	8.395162	-0.055916	4.388539
280.064675	6612.179901	8.400166	-0.055964	4.391127
280.240276	6620.212683	8.405171	-0.056002	4.393702
280.324109	6628.274220	8.410176	-0.056022	4.396285
280.417369	6636.201866	8.415181	-0.056045	4.398824
280.423692	6644.230237	8.420186	-0.056051	4.401393
280.829797	6652.222642	8.425190	-0.056131	4.403950
281.108863	6660.230693	8.430195	-0.056188	4.406511
281.277694	6668.258954	8.435200	-0.056225	4.409076
281.376463	6676.296973	8.440205	-0.056248	4.411642
281.556528	6684.312033	8.445210	-0.056286	4.414200
281.471981	6692.381891	8.450214	-0.056276	4.416773
281.792217	6700.319008	8.455219	-0.056340	4.419304
281.820332	6708.393610	8.460224	-0.056351	4.421875
281.930899	6716.339261	8.465229	-0.056376	4.424405
282.213499	6724.438211	8.470234	-0.056434	4.426982
282.457598	6732.436459	8.475238	-0.056484	4.429526
282.425507	6740.489493	8.480243	-0.056483	4.432084
282.884321	6748.557080	8.485248	-0.056574	4.434648
283.025530	6756.520706	8.490253	-0.056605	4.437176
283.214572	6764.493214	8.495258	-0.056645	4.439705
283.371301	6772.521024	8.500262	-0.056679	4.442251
283.438076	6780.433440	8.505267	-0.056696	4.444758
283.704018	6788.531238	8.510272	-0.056751	4.447323
283.715936	6796.555142	8.515277	-0.056758	4.449862
283.739645	6804.638791	8.520282	-0.056768	4.452419
284.098772	6812.632073	8.525286	-0.056839	4.454946
284.107768	6820.645163	8.530291	-0.056846	4.457478
284.418099	6828.635485	8.535296	-0.056909	4.460002
284.635641	6836.646396	8.540301	-0.056954	4.462530
284.868118	6844.627113	8.545306	-0.057002	4.465048
285.064884	6852.683188	8.550310	-0.057044	4.467587
285.184168	6860.683328	8.555315	-0.057071	4.470108
285.544171	6868.740952	8.560320	-0.057143	4.472646
285.575964	6876.760184	8.565325	-0.057154	4.475169
285.610952	6884.750162	8.570330	-0.057166	4.477682
285.959478	6892.763257	8.575335	-0.057235	4.480201
285.791621	6900.750471	8.580339	-0.057209	4.482709
286.121184	6908.755039	8.585344	-0.057275	4.485223
286.211329	6916.779518	8.590349	-0.057297	4.487741
286.600848	6924.794720	8.595354	-0.057375	4.490255
286.692951	6932.851251	8.600359	-0.057397	4.492780
286.839814	6940.846049	8.605363	-0.057429	4.495285
287.060950	6948.885603	8.610368	-0.057475	4.497802
287.242066	6956.862232	8.615373	-0.057514	4.500298
287.416496	6964.885373	8.620378	-0.057551	4.502807
287.525580	6972.880638	8.625383	-0.057577	4.505306
287.677500	6980.920034	8.630387	-0.057610	4.507818
287.802473	6988.949191	8.635392	-0.057638	4.510324
288.065028	6997.033843	8.640397	-0.057692	4.512847
288.237871	7005.068732	8.645402	-0.057729	4.515353
288.349211	7013.040473	8.650407	-0.057755	4.517837
288.394133	7020.953967	8.655411	-0.057768	4.520302
288.532929	7029.015605	8.660416	-0.057799	4.522812
288.557365	7036.996243	8.665421	-0.057809	4.525295
288.718560	7045.050672	8.670426	-0.057844	4.527800
288.996302	7053.025470	8.675431	-0.057900	4.530279
289.057053	7061.094595	8.680435	-0.057916	4.532785
289.252807	7069.118101	8.685440	-0.057958	4.535276
289.467366	7077.105729	8.690445	-0.058003	4.537754
289.727354	7085.070365	8.695450	-0.058056	4.540225
289.620991	7093.175483	8.700455	-0.058041	4.542736
289.587904	7101.116290	8.705459	-0.058040	4.545196
290.126640	7109.223907	8.710464	-0.058145	4.547706
290.278531	7117.159473	8.715469	-0.058179	4.550162
290.408711	7125.227750	8.720474	-0.058208	4.552657
290.525551	7133.244998	8.725479	-0.058235	4.555135
290.440714	7141.270571	8.730483	-0.058224	4.557614
290.768598	7149.253259	8.735488	-0.058290	4.560079
291.099387	7157.288971	8.740493	-0.058356	4.562558
291.108484	7165.258499	8.745498	-0.058363	4.565016
291.195409	7173.349588	8.750503	-0.058384	4.567510
291.413837	7181.294661	8.755507	-0.058430	4.569958
291.620996	7189.367869	8.760512	-0.058473	4.572443
291.849934	7197.349080	8.765517	-0.058521	4.574899
291.763799	7205.453340	8.770522	-0.058510	4.577392
292.070167	7213.415693	8.775527	-0.058572	4.579839
292.264357	7221.451824	8.780531	-0.058613	4.582308
292.559455	7229.445365	8.785536	-0.058673	4.584763
292.900300	7237.429992	8.790541	-0.058741	4.587213
293.207240	7245.460835	8.795546	-0.058803	4.589677
293.452521	7253.503350	8.800551	-0.058854	4.592142
293.324564	7261.557950	8.805555	-0.058835	4.594610
293.589204	7269.601065	8.810560	-0.058890	4.597073
293.832279	7277.502708	8.815565	-0.058940	4.599491
293.867973	7285.552734	8.820570	-0.058951	4.601953
293.978766	7293.538606	8.825575	-0.058977	4.604395
294.155734	7301.584950	8.830579	-0.059015	4.606853
294.374151	7309.608048	8.835584	-0.059060	4.609303
294.479566	7317.581287	8.840589	-0.059085	4.611737
294.737245	7325.629443	8.845594	-0.059138	4.614192
294.928068	7333.699382	8.850599	-0.059179	4.616652
294.962644	7341.627078	8.855603	-0.059190	4.619068
295.198528	7349.704690	8.860608	-0.059239	4.621528
295.553743	7357.625753	8.865613	-0.059310	4.623940
295.735536	7365.723340	8.870618	-0.059349	4.626403
296.048177	7373.749497	8.875623	-0.059412	4.628844
296.112690	7381.716964	8.880627	-0.059429	4.631265
296.157995	7389.783182	8.885632	-0.059442	4.633715
296.093499	7397.797940	8.890637	-0.059435	4.636148
296.379572	7405.765140	8.895642	-0.059493	4.638566
296.706954	7413.778927	8.900647	-0.059559	4.640996
296.844456	7421.768759	8.905651	-0.059590	4.643418
297.163780	7429.824127	8.910656	-0.059654	4.645858
297.462863	7437.839457	8.915661	-0.059715	4.648285
297.493804	7445.855178	8.920666	-0.059726	4.650710
297.582660	7453.895941	8.925671	-0.059747	4.653142
297.888869	7461.866299	8.930675	-0.059809	4.655552
298.177502	7469.932830	8.935680	-0.059868	4.657989
298.149277	7477.891839	8.940685	-0.059868	4.660392
298.594063	7485.917910	8.945690	-0.059955	4.662814
298.639830	7493.896952	8.950695	-0.059969	4.665221
298.902254	7501.981564	8.955699	-0.060023	4.667659
299.000425	7510.003431	8.960704	-0.060046	4.670076
299.269834	7518.045878	8.965709	-0.060101	4.672498
299.604113	7526.125094	8.970714	-0.060168	4.674930
299.767248	7534.126807	8.975719	-0.060204	4.677337
299.962609	7541.985434	8.980723	-0.060245	4.679700
300.290010	7550.076381	8.985728	-0.060311	4.682132
300.461862	7558.027317	8.990733	-0.060348	4.684520
300.797164	7566.098808	8.995738	-0.060415	4.686943
301.325304	7574.067590	9.000743	-0.060519	4.689334
301.095092	7582.123250	9.005747	-0.060481	4.691750
301.371331	7590.152989	9.010752	-0.060537	4.694157
301.508662	7598.176641	9.015757	-0.060568	4.696561
301.740536	7606.149859	9.020762	-0.060616	4.698948
301.962590	7614.174105	9.025767	-0.060662	4.701350
302.070863	7622.139081	9.030771	-0.060687	4.703733
302.138681	7630.210181	9.035776	-0.060705	4.706146
302.345298	7638.236383	9.040781	-0.060748	4.708544
302.543580	7646.218608	9.045786	-0.060790	4.710928
302.699484	7654.310255	9.050791	-0.060824	4.713344
302.817881	7662.271858	9.055795	-0.060851	4.715719
303.047756	7670.322241	9.060800	-0.060899	4.718120
303.268670	7678.312842	9.065805	-0.060945	4.720501
303.391169	7686.315075	9.070810	-0.060973	4.722885
303.568475	7694.332392	9.075815	-0.061011	4.725272
303.634091	7702.373781	9.080819	-0.061028	4.727666
303.960021	7710.360873	9.085824	-0.061094	4.730041
303.923176	7718.402151	9.090829	-0.061092	4.732432
304.159657	7726.443891	9.095834	-0.061141	4.734821
304.454496	7734.451484	9.100839	-0.061201	4.737199
304.394804	7742.403823	9.105843	-0.061194	4.739560
304.628854	7750.466325	9.110848	-0.061243	4.741952
304.722009	7758.424094	9.115853	-0.061265	4.744312
304.770177	7766.518109	9.120858	-0.061279	4.746711
304.929760	7774.494167	9.125863	-0.061314	4.749074
304.978268	7782.498322	9.130867	-0.061328	4.751444
305.334483	7790.597593	9.135872	-0.061399	4.753840
305.407464	7798.585904	9.140877	-0.061418	4.756203
305.606737	7806.532196	9.145882	-0.061460	4.758552
305.630033	7814.576529	9.150887	-0.061469	4.760930
305.762153	7822.546946	9.155891	-0.061499	4.763284
306.062290	7830.560472	9.160896	-0.061560	4.765649
306.133366	7838.576265	9.165901	-0.061578	4.768014
306.371197	7846.614093	9.170906	-0.061627	4.770384
306.381009	7854.671055	9.175911	-0.061634	4.772759
306.566759	7862.655943	9.180915	-0.061673	4.775111
306.636582	7870.693126	9.185920	-0.061691	4.777478
306.723335	7878.683638	9.190925	-0.061712	4.779830
307.015625	7886.686270	9.195930	-0.061772	4.782183
307.257305	7894.686945	9.200935	-0.061822	4.784535
307.369327	7902.711065	9.205939	-0.061848	4.786893
307.530990	7910.751599	9.210944	-0.061883	4.789254
307.566177	7918.744342	9.215949	-0.061894	4.791601
307.854376	7926.800092	9.220954	-0.061953	4.793964
307.918335	7934.873610	9.225959	-0.061970	4.796332
307.987625	7942.778690	9.230963	-0.061988	4.798650
308.361767	7950.830833	9.235968	-0.062062	4.801008
308.617762	7958.836207	9.240973	-0.062115	4.803351
308.570701	7966.794955	9.245978	-0.062111	4.805682
308.848457	7974.885460	9.250983	-0.062168	4.808048
308.626717	7982.863097	9.255987	-0.062131	4.810382
308.816245	7990.292581	9.260992	-0.062171	4.812553
309.042781	7994.753335	9.265997	-0.062216	4.813856
309.237248	7997.216335	9.271002	-0.062254	4.814574
309.440217	7998.567278	9.276007	-0.062292	4.814968
309.239107	7998.951885	9.281011	-0.062255	4.815081
309.538071	7999.904825	9.286016	-0.062311	4.815358
309.480152	7999.917737	9.291021	-0.062300	4.815362
309.542299	7999.908055	9.296026	-0.062311	4.815359
309.878166	7999.951003	9.301031	-0.062373	4.815370
309.810044	7999.877172	9.306035	-0.062360	4.815349
309.823051	7999.910498	9.311040	-0.062362	4.815359
309.837655	7999.883996	9.316045	-0.062365	4.815351
310.185254	7999.890798	9.321050	-0.062429	4.815351
310.209147	7999.942475	9.326055	-0.062434	4.815366
310.236116	7999.893732	9.331059	-0.062438	4.815352
310.385896	7999.914361	9.336064	-0.062466	4.815357
310.347777	7999.936152	9.341069	-0.062459	4.815364
310.452252	7999.929309	9.346074	-0.062478	4.815361
310.688548	7999.909686	9.351079	-0.062522	4.815354
310.470787	7999.864370	9.356083	-0.062481	4.815342
310.586147	7999.890842	9.361088	-0.062502	4.815349
310.554784	7999.906332	9.366093	-0.062496	4.815354
310.582352	7999.926005	9.371098	-0.062501	4.815360
310.714778	7999.897179	9.376103	-0.062525	4.815350
310.523490	7999.855509	9.381107	-0.062489	4.815339
310.712569	7999.898165	9.386112	-0.062524	4.815351
310.701410	7999.926817	9.391117	-0.062522	4.815359
310.733959	7999.900612	9.396122	-0.062528	4.815351
310.692091	7999.923410	9.401127	-0.062520	4.815358
310.659477	7999.876886	9.406131	-0.062513	4.815345
310.793325	7999.875874	9.411136	-0.062538	4.815344
310.675392	7999.886723	9.416141	-0.062516	4.815348
311.049903	7999.899318	9.421146	-0.062585	4.815350
311.044834	7999.939828	9.426151	-0.062584	4.815361
310.890308	7999.859218	9.431155	-0.062555	4.815339
311.121065	7999.917530	9.436160	-0.062598	4.815355
311.223006	7999.886061	9.441165	-0.062616	4.815345
311.296942	7999.876575	9.446170	-0.062630	4.815342
311.204727	7999.882506	9.451175	-0.062612	4.815344
311.257380	7999.875873	9.456179	-0.062622	4.815342
311.152303	7999.963894	9.461184	-0.062602	4.815368
310.977800	7999.991976	9.466189	-0.062569	4.815377
311.009132	7999.939029	9.471194	-0.062575	4.815361
310.984662	8000.028385	9.476199	-0.062570	4.815388
311.025942	7999.932849	9.481203	-0.062578	4.815360
311.094347	7999.939304	9.486208	-0.062590	4.815361
311.076329	7999.899434	9.491213	-0.062586	4.815350
311.127792	7999.940881	9.496218	-0.062596	4.815361
311.042975	7999.973656	9.501223	-0.062580	4.815371
310.904474	7999.902931	9.506227	-0.062554	4.815351
311.160961	7999.923191	9.511232	-0.062601	4.815356
311.149829	7999.906950	9.516237	-0.062599	4.815351
311.143693	7999.915377	9.521242	-0.062597	4.815354
311.236311	7999.994915	9.526247	-0.062615	4.815377
311.204910	7999.953755	9.531251	-0.062608	4.815365
311.304313	7999.973550	9.536256	-0.062627	4.815370
311.342506	7999.936750	9.541261	-0.062633	4.815359
311.394897	7999.915149	9.546266	-0.062643	4.815353
311.318965	7999.924556	9.551271	-0.062629	4.815356
311.332012	7999.878788	9.556275	-0.062631	4.815342
311.408838	7999.934550	9.561280	-0.062645	4.815358
311.441802	7999.939349	9.566285	-0.062651	4.815360
311.319573	7999.920199	9.571290	-0.062628	4.815355
311.672528	7999.968780	9.576295	-0.062693	4.815367
311.563191	7999.903881	9.581299	-0.062673	4.815349
311.495473	7999.931596	9.586304	-0.062660	4.815357
311.454005	7999.937299	9.591309	-0.062652	4.815359
311.459792	7999.907443	9.596314	-0.062652	4.815350
311.355190	7999.964475	9.601319	-0.062633	4.815367
311.644048	7999.897624	9.606323	-0.062686	4.815346
311.790007	7999.932087	9.611328	-0.062713	4.815356
311.708956	7999.952098	9.616333	-0.062698	4.815362
311.686978	7999.928195	9.621338	-0.062694	4.815355
311.817593	7999.982712	9.626343	-0.062718	4.815370
311.695150	7999.934698	9.631347	-0.062695	4.815357
311.786339	7999.958633	9.636352	-0.062711	4.815364
311.652800	7999.967085	9.641357	-0.062686	4.815367
311.588028	7999.909339	9.646362	-0.062674	4.815350
311.842004	7999.928489	9.651367	-0.062721	4.815355
311.695071	7999.916411	9.656371	-0.062693	4.815352
311.928965	7999.946986	9.661376	-0.062737	4.815360
311.948341	8000.009280	9.666381	-0.062740	4.815378
311.886323	7999.980438	9.671386	-0.062728	4.815370
312.020695	8000.001882	9.676391	-0.062753	4.815375
311.829101	7999.973030	9.681395	-0.062717	4.815368
311.968574	7999.944321	9.686400	-0.062743	4.815359
312.019925	7999.957976	9.691405	-0.062752	4.815362
312.016906	7999.944008	9.696410	-0.062751	4.815358
312.001941	7999.959770	9.701415	-0.062748	4.815363
311.849260	7999.943321	9.706419	-0.062719	4.815359
311.824476	7999.965334	9.711424	-0.062714	4.815365
311.719091	7999.968908	9.716429	-0.062695	4.815367
311.710870	7999.936683	9.721434	-0.062693	4.815358
311.749826	7999.936237	9.726439	-0.062700	4.815357
311.754460	7999.891398	9.731443	-0.062700	4.815344
311.883586	7999.937339	9.736448	-0.062724	4.815357
311.720479	7999.950646	9.741453	-0.062694	4.815362
311.921192	7999.947536	9.746458	-0.062731	4.815360
311.790419	7999.944277	9.751463	-0.062706	4.815360
311.723098	7999.873661	9.756467	-0.062693	4.815339
311.871647	7999.924199	9.761472	-0.062721	4.815353
311.955130	7999.986486	9.766477	-0.062736	4.815371
312.010811	7999.968146	9.771482	-0.062746	4.815365
311.896856	7999.935237	9.776487	-0.062725	4.815356
311.803279	7999.903735	9.781491	-0.062707	4.815348
312.039134	7999.935412	9.786496	-0.062751	4.815356
312.121782	7999.959205	9.791501	-0.062766	4.815362
311.767067	7999.910548	9.796506	-0.062699	4.815350
311.814178	7999.975438	9.801511	-0.062708	4.815369
311.858104	7999.947284	9.806515	-0.062716	4.815360
312.091354	7999.952196	9.811520	-0.062759	4.815360
311.870004	7999.951710	9.816525	-0.062718	4.815361
311.765626	7999.907202	9.821530	-0.062698	4.815349
311.892873	7999.936010	9.826535	-0.062721	4.815357
311.792421	7999.922565	9.831539	-0.062702	4.815353
312.091196	7999.918943	9.836544	-0.062758	4.815351
312.173725	7999.902117	9.841549	-0.062773	4.815345
312.166077	7999.908380	9.846554	-0.062771	4.815347
312.025233	7999.930607	9.851559	-0.062745	4.815355
311.985240	7999.956643	9.856563	-0.062737	4.815362
312.188678	7999.946097	9.861568	-0.062775	4.815358
312.278508	7999.931530	9.866573	-0.062791	4.815354
312.047105	7999.928740	9.871578	-0.062748	4.815354
312.291082	7999.945588	9.876583	-0.062793	4.815358
312.166184	7999.887912	9.881587	-0.062769	4.815341
312.070290	7999.941882	9.886592	-0.062751	4.815358
312.073218	7999.928012	9.891597	-0.062751	4.815354
312.124733	7999.939532	9.896602	-0.062761	4.815357
312.104840	7999.971246	9.901607	-0.062757	4.815366
312.128029	7999.961987	9.906611	-0.062761	4.815363
312.340992	7999.962288	9.911616	-0.062800	4.815362
312.345103	7999.939886	9.916621	-0.062801	4.815356
312.204588	7999.927914	9.921626	-0.062774	4.815353
312.328665	8000.001563	9.926631	-0.062797	4.815374
312.367007	7999.936973	9.931635	-0.062804	4.815355
312.294844	7999.962477	9.936640	-0.062790	4.815363
312.525826	7999.971627	9.941645	-0.062833	4.815364
312.237693	7999.934761	9.946650	-0.062779	4.815355
312.307097	8000.000022	9.951655	-0.062792	4.815374
312.366213	7999.973188	9.956659	-0.062803	4.815365
312.204097	8000.002544	9.961664	-0.062772	4.815375
312.462624	8000.016427	9.966669	-0.062820	4.815378
312.439044	7999.971120	9.971674	-0.062816	4.815365
312.466399	7999.976895	9.976679	-0.062820	4.815366
312.335843	7999.934089	9.981683	-0.062796	4.815354
312.301021	7999.927076	9.986688	-0.062789	4.815352
312.434046	7999.944222	9.991693	-0.062814	4.815357
312.432569	7999.938831	9.996698	-0.062813	4.815355
312.554925	7999.965421	10.001703	-0.062836	4.815362
312.512356	7999.956141	10.006707	-0.062827	4.815360
312.399251	7999.935003	10.011712	-0.062806	4.815354
312.364059	8000.003874	10.016717	-0.062799	4.815375
312.260549	7999.913417	10.021722	-0.062780	4.815349
312.457569	7999.977587	10.026727	-0.062816	4.815366
312.477757	7999.935143	10.031731	-0.062820	4.815354
312.589323	7999.930556	10.036736	-0.062840	4.815352
312.498717	7999.925825	10.041741	-0.062823	4.815351
312.569760	7999.882086	10.046746	-0.062836	4.815338
312.743847	7999.964047	10.051751	-0.062868	4.815361
312.485649	7999.959744	10.056755	-0.062820	4.815361
312.534006	7999.908147	10.061760	-0.062828	4.815346
312.471296	7999.957322	10.066765	-0.062817	4.815360
312.456208	7999.911087	10.071770	-0.062813	4.815347
312.615594	7999.956462	10.076775	-0.062843	4.815360
312.830892	7999.918321	10.081779	-0.062883	4.815347
312.700112	7999.962092	10.086784	-0.062858	4.815361
312.594940	7999.964601	10.091789	-0.062838	4.815362
312.685657	7999.943636	10.096794	-0.062855	4.815355
312.619081	7999.989540	10.101799	-0.062842	4.815369
312.467422	7999.965625	10.106803	-0.062814	4.815363
312.542290	7999.989290	10.111808	-0.062828	4.815370
312.806651	8000.050302	10.116813	-0.062877	4.815386
312.629427	7999.942588	10.121818	-0.062843	4.815355
312.545067	7999.979647	10.126823	-0.062827	4.815367
312.538067	7999.958130	10.131827	-0.062826	4.815360
312.567438	7999.963939	10.136832	-0.062831	4.815362
312.540715	7999.978437	10.141837	-0.062826	4.815366
312.680619	7999.946529	10.146842	-0.062851	4.815356
312.755824	7999.993716	10.151847	-0.062865	4.815370
312.703061	7999.940442	10.156851	-0.062855	4.815355
312.737833	7999.937788	10.161856	-0.062861	4.815354
312.659150	7999.962115	10.166861	-0.062846	4.815361
312.628149	7999.918822	10.171866	-0.062840	4.815349
312.747118	7999.969940	10.176871	-0.062862	4.815363
312.783162	7999.963033	10.181875	-0.062869	4.815361
312.803519	7999.999690	10.186880	-0.062872	4.815371
312.793741	8000.023021	10.191885	-0.062870	4.815378
312.683933	7999.980559	10.196890	-0.062849	4.815366
312.857559	8000.051825	10.201895	-0.062882	4.815386
312.551215	7999.978313	10.206899	-0.062824	4.815366
312.741199	7999.934408	10.211904	-0.062859	4.815353
312.979543	7999.936199	10.216909	-0.062903	4.815352
312.862276	7999.951334	10.221914	-0.062881	4.815357
312.807268	8000.008120	10.226919	-0.062871	4.815374
312.871983	7999.976034	10.231923	-0.062883	4.815364
312.844556	7999.959522	10.236928	-0.062877	4.815360
312.737024	7999.978026	10.241933	-0.062857	4.815365
312.655740	7999.922141	10.246938	-0.062842	4.815350
312.868523	7999.981229	10.251943	-0.062881	4.815366
312.823878	7999.929158	10.256947	-0.062872	4.815351
312.708942	7999.944332	10.261952	-0.062851	4.815356
312.831111	7999.957024	10.266957	-0.062873	4.815359
312.733630	7999.940420	10.271962	-0.062855	4.815355
313.003788	7999.991908	10.276967	-0.062905	4.815368
313.048761	7999.963770	10.281971	-0.062913	4.815360
313.098847	7999.972060	10.286976	-0.062922	4.815362
313.010831	8000.005852	10.291981	-0.062905	4.815372
313.035690	7999.946382	10.296986	-0.062910	4.815355
313.217972	7999.992138	10.301991	-0.062944	4.815367
313.189943	7999.990581	10.306995	-0.062938	4.815367
312.995568	7999.947786	10.312000	-0.062902	4.815355
313.235210	7999.967770	10.317005	-0.062946	4.815360
313.288881	7999.932294	10.322010	-0.062956	4.815350
313.271106	7999.950148	10.327015	-0.062952	4.815355
313.178726	7999.965696	10.332019	-0.062935	4.815360
313.417047	7999.943971	10.337024	-0.062979	4.815352
313.282337	7999.972712	10.342029	-0.062953	4.815361
313.433270	7999.933505	10.347034	-0.062981	4.815349
313.461713	7999.994882	10.352039	-0.062986	4.815367
313.362968	7999.965429	10.357043	-0.062968	4.815359
313.383197	7999.918709	10.362048	-0.062971	4.815345
313.468562	7999.914758	10.367053	-0.062987	4.815344
313.422315	7999.908623	10.372058	-0.062978	4.815342
313.247445	7999.959146	10.377063	-0.062945	4.815358
313.297501	7999.961022	10.382067	-0.062954	4.815358
313.315664	7999.958093	10.387072	-0.062957	4.815357
313.304547	7999.922612	10.392077	-0.062955	4.815347
313.179028	7999.922645	10.397082	-0.062931	4.815347
313.470952	7999.960600	10.402087	-0.062985	4.815357
313.292478	7999.985409	10.407091	-0.062952	4.815365
313.493529	7999.945963	10.412096	-0.062989	4.815353
313.458093	7999.927181	10.417101	-0.062982	4.815347
313.331976	7999.956065	10.422106	-0.062959	4.815356
313.358608	7999.981069	10.427111	-0.062963	4.815364
313.321638	7999.959054	10.432115	-0.062956	4.815357
313.547467	7999.965983	10.437120	-0.062998	4.815358
313.642279	8000.025255	10.442125	-0.063015	4.815375
313.417126	7999.973396	10.447130	-0.062973	4.815361
313.568608	7999.994057	10.452135	-0.063001	4.815366
313.459133	7999.923808	10.457139	-0.062980	4.815346
313.289675	7999.977627	10.462144	-0.062949	4.815363
313.299163	7999.975623	10.467149	-0.062950	4.815362
313.427776	7999.943528	10.472154	-0.062974	4.815352
313.478913	7999.965731	10.477159	-0.062983	4.815359
313.357227	7999.941243	10.482163	-0.062960	4.815352
313.393398	7999.935407	10.487168	-0.062967	4.815350
313.602694	8000.002990	10.492173	-0.063005	4.815369
313.411144	7999.961309	10.497178	-0.062969	4.815358
313.511846	7999.954405	10.502183	-0.062988	4.815355
313.466485	7999.934389	10.507187	-0.062979	4.815350
313.327951	7999.970549	10.512192	-0.062953	4.815361
313.467252	8000.013455	10.517197	-0.062979	4.815373
313.451718	7999.907352	10.522202	-0.062976	4.815342
313.509326	8000.004487	10.527207	-0.062986	4.815370
313.503138	7999.975501	10.532211	-0.062985	4.815361
313.443336	7999.934936	10.537216	-0.062973	4.815350
313.509005	7999.989448	10.542221	-0.062985	4.815365
313.535252	7999.952448	10.547226	-0.062990	4.815355
313.424706	7999.955936	10.552231	-0.062969	4.815356
313.568217	7999.918743	10.557235	-0.062996	4.815345
313.713854	7999.955341	10.562240	-0.063022	4.815355
313.693130	7999.969939	10.567245	-0.063018	4.815359
313.602741	7999.910696	10.572250	-0.063001	4.815342
313.694286	7999.930363	10.577255	-0.063018	4.815347
313.763993	7999.961425	10.582259	-0.063031	4.815356
313.762022	7999.917544	10.587264	-0.063030	4.815343
313.734487	7999.924547	10.592269	-0.063025	4.815345
313.588950	7999.917834	10.597274	-0.062997	4.815344
313.737869	7999.959831	10.602279	-0.063025	4.815356
313.699144	7999.937788	10.607283	-0.063017	4.815350
313.659356	7999.934967	10.612288	-0.063010	4.815349
313.613326	7999.919216	10.617293	-0.063001	4.815345
313.529733	7999.901773	10.622298	-0.062985	4.815340
313.640547	7999.954895	10.627303	-0.063005	4.815355
313.511013	7999.904623	10.632307	-0.062981	4.815341
313.618533	7999.925624	10.637312	-0.063001	4.815346
313.842046	7999.980616	10.642317	-0.063042	4.815361
313.675125	7999.930792	10.647322	-0.063011	4.815348
313.735731	7999.964911	10.652327	-0.063022	4.815357
313.680565	7999.969317	10.657331	-0.063011	4.815359
313.544657	7999.936042	10.662336	-0.062986	4.815350
313.919314	7999.951853	10.667341	-0.063055	4.815353
313.713704	7999.915283	10.672346	-0.063017	4.815343
313.963399	7999.974985	10.677351	-0.063063	4.815359
313.894791	7999.942826	10.682355	-0.063050	4.815350
313.955718	7999.944882	10.687360	-0.063061	4.815350
314.084005	7999.960883	10.692365	-0.063085	4.815355
313.851978	7999.919599	10.697370	-0.063041	4.815344
313.944671	7999.955319	10.702375	-0.063058	4.815354
313.871115	7999.944456	10.707379	-0.063044	4.815351
313.663713	7999.918546	10.712384	-0.063005	4.815344
313.714267	7999.980290	10.717389	-0.063014	4.815362
313.713520	7999.953531	10.722394	-0.063014	4.815354
313.580666	7999.975890	10.727399	-0.062989	4.815361
313.529314	7999.991049	10.732403	-0.062979	4.815366
313.453868	7999.981223	10.737408	-0.062965	4.815364
313.656667	8000.018769	10.742413	-0.063003	4.815374
313.817299	7999.947655	10.747418	-0.063032	4.815352
313.724276	7999.974950	10.752423	-0.063015	4.815360
313.687987	7999.937982	10.757427	-0.063008	4.815350
313.721513	7999.991961	10.762432	-0.063014	4.815365
313.609220	8000.038177	10.767437	-0.062992	4.815380
313.657854	7999.982308	10.772442	-0.063001	4.815363
313.832494	7999.973423	10.777447	-0.063033	4.815360
313.940883	7999.978405	10.782451	-0.063053	4.815360
313.828118	7999.964753	10.787456	-0.063032	4.815357
313.570111	7999.965796	10.792461	-0.062984	4.815359
313.684645	7999.951638	10.797466	-0.063005	4.815354
313.809156	7999.983610	10.802471	-0.063028	4.815363
313.691762	7999.997674	10.807475	-0.063006	4.815367
313.803803	7999.947132	10.812480	-0.063026	4.815352
313.834500	8000.001065	10.817485	-0.063032	4.815368
313.622037	7999.946210	10.822490	-0.062992	4.815353
313.894935	7999.985987	10.827495	-0.063042	4.815363
313.838673	7999.974342	10.832499	-0.063032	4.815360
313.846189	7999.966961	10.837504	-0.063033	4.815358
313.828814	8000.012613	10.842509	-0.063029	4.815371
313.779820	7999.945505	10.847514	-0.063020	4.815352
313.802250	8000.033505	10.852519	-0.063024	4.815377
313.898625	8000.035081	10.857523	-0.063042	4.815377
313.809052	8000.004711	10.862528	-0.063025	4.815369
313.744602	7999.997206	10.867533	-0.063012	4.815367
313.659497	7999.985082	10.872538	-0.062996	4.815364
313.779873	8000.030881	10.877543	-0.063018	4.815377
313.917774	8000.024594	10.882547	-0.063044	4.815374
313.701240	7999.987843	10.887552	-0.063003	4.815365
313.820954	7999.990875	10.892557	-0.063025	4.815365
313.854554	7999.948652	10.897562	-0.063031	4.815352
313.989020	7999.988272	10.902567	-0.063056	4.815363
314.010095	8000.014253	10.907571	-0.063060	4.815371
313.773109	7999.967542	10.912576	-0.063015	4.815358
313.736180	8000.001112	10.917581	-0.063008	4.815368
313.733311	7999.906976	10.922586	-0.063007	4.815341
313.818976	7999.952200	10.927591	-0.063023	4.815354
313.888092	7999.980046	10.932595	-0.063036	4.815361
313.867615	7999.968994	10.937600	-0.063032	4.815358
313.976745	7999.971850	10.942605	-0.063052	4.815359
313.931392	7999.972144	10.947610	-0.063043	4.815359
313.874977	8000.034252	10.952615	-0.063032	4.815377
313.930511	7999.982773	10.957619	-0.063042	4.815362
313.951564	7999.940342	10.962624	-0.063046	4.815350
313.953986	7999.966013	10.967629	-0.063046	4.815357
313.870551	7999.985985	10.972634	-0.063030	4.815363
313.879470	8000.026729	10.977639	-0.063032	4.815375
313.902005	8000.032424	10.982643	-0.063036	4.815377
313.781186	7999.961986	10.987648	-0.063013	4.815357
313.968839	7999.985385	10.992653	-0.063048	4.815363
314.014228	7999.928393	10.997658	-0.063056	4.815346
314.019020	7999.980827	11.002663	-0.063057	4.815361
314.072272	7999.990239	11.007667	-0.063066	4.815364
314.029468	7999.951024	11.012672	-0.063058	4.815352
313.898478	7999.942415	11.017677	-0.063033	4.815350
313.926416	7999.931098	11.022682	-0.063038	4.815347
314.063430	7999.968622	11.027687	-0.063064	4.815357
314.124631	7999.982441	11.032691	-0.063075	4.815361
313.818998	7999.975211	11.037696	-0.063017	4.815360
314.024906	8000.029912	11.042701	-0.063056	4.815375
314.092245	7999.944422	11.047706	-0.063068	4.815350
313.896137	7999.970008	11.052711	-0.063031	4.815359
313.872393	8000.001659	11.057715	-0.063026	4.815368
313.862682	7999.975820	11.062720	-0.063024	4.815360
313.955129	8000.052156	11.067725	-0.063041	4.815382
313.850178	7999.931741	11.072730	-0.063021	4.815348
313.983603	7999.969206	11.077735	-0.063046	4.815358
313.993612	7999.945832	11.082739	-0.063048	4.815351
314.159761	7999.975288	11.087744	-0.063078	4.815359
314.191378	8000.035650	11.092749	-0.063084	4.815376
313.828722	7999.957993	11.097754	-0.063016	4.815355
313.848944	8000.010683	11.102759	-0.063020	4.815371
313.965626	7999.966632	11.107763	-0.063041	4.815357
313.923061	7999.978730	11.112768	-0.063033	4.815361
313.868760	7999.990633	11.117773	-0.063023	4.815365
313.877721	7999.967242	11.122778	-0.063024	4.815358
314.006558	7999.968287	11.127783	-0.063048	4.815358
313.987140	7999.991459	11.132787	-0.063044	4.815365
313.891979	7999.940687	11.137792	-0.063026	4.815350
314.080317	8000.015406	11.142797	-0.063061	4.815371
314.066198	7999.954220	11.147802	-0.063058	4.815353
314.004274	7999.958514	11.152807	-0.063046	4.815355
313.927384	7999.942251	11.157811	-0.063031	4.815350
314.049728	7999.972049	11.162816	-0.063054	4.815359
314.012968	8000.024863	11.167821	-0.063047	4.815374
314.048429	7999.967706	11.172826	-0.063053	4.815357
314.183153	8000.015882	11.177831	-0.063078	4.815371
314.075126	8000.040790	11.182835	-0.063058	4.815379
314.034601	7999.949236	11.187840	-0.063050	4.815352
314.237179	8000.042364	11.192845	-0.063087	4.815378
314.045116	7999.937606	11.197850	-0.063051	4.815349
313.897525	7999.978961	11.202855	-0.063024	4.815361
313.815201	8000.025674	11.207859	-0.063008	4.815375
313.896083	7999.970340	11.212864	-0.063023	4.815359
314.065158	7999.994500	11.217869	-0.063054	4.815365
313.881221	7999.948669	11.222874	-0.063019	4.815353
313.985755	7999.947173	11.227879	-0.063039	4.815352
314.029610	7999.999186	11.232883	-0.063047	4.815367
313.995473	7999.998597	11.237888	-0.063040	4.815367
314.148647	8000.052423	11.242893	-0.063068	4.815382
314.228155	7999.985308	11.247898	-0.063083	4.815362
314.200777	8000.044691	11.252903	-0.063078	4.815379
314.174417	8000.015369	11.257907	-0.063072	4.815371
314.179082	7999.976942	11.262912	-0.063073	4.815360
314.151977	8000.010675	11.267917	-0.063068	4.815370
313.972627	7999.956369	11.272922	-0.063034	4.815355
314.141486	8000.005110	11.277927	-0.063065	4.815368
314.182669	7999.989737	11.282931	-0.063073	4.815363
314.161028	7999.996837	11.287936	-0.063068	4.815365
314.094384	7999.994640	11.292941	-0.063056	4.815365
314.226934	7999.938024	11.297946	-0.063080	4.815348
314.387417	7999.999455	11.302951	-0.063110	4.815365
314.157721	8000.040517	11.307955	-0.063067	4.815378
314.189188	7999.979018	11.312960	-0.063072	4.815360
314.468695	8000.039216	11.317965	-0.063124	4.815376
314.326234	7999.954522	11.322970	-0.063097	4.815352
314.361515	8000.016013	11.327975	-0.063104	4.815370
314.454601	8000.059223	11.332979	-0.063121	4.815382
314.479650	7999.945239	11.337984	-0.063125	4.815349
314.392222	8000.028212	11.342989	-0.063109	4.815374
314.504761	7999.947748	11.347994	-0.063129	4.815350
314.629343	7999.989342	11.352999	-0.063152	4.815361
314.560028	7999.994583	11.358003	-0.063139	4.815363
314.284491	7999.981437	11.363008	-0.063087	4.815360
314.352952	8000.016756	11.368013	-0.063100	4.815370
314.261949	7999.960708	11.373018	-0.063083	4.815355
314.334950	7999.993964	11.378023	-0.063096	4.815364
314.196337	8000.007675	11.383027	-0.063070	4.815369
314.161511	7999.964318	11.388032	-0.063063	4.815356
314.123950	8000.006429	11.393037	-0.063056	4.815369
314.237470	7999.975152	11.398042	-0.063077	4.815359
314.232684	8000.024220	11.403047	-0.063076	4.815373
314.139380	8000.026925	11.408051	-0.063058	4.815375
314.260265	8000.002184	11.413056	-0.063080	4.815367
314.365282	8000.027420	11.418061	-0.063100	4.815374
314.392060	7999.988291	11.423066	-0.063104	4.815362
314.307730	7999.971904	11.428071	-0.063088	4.815358
314.471233	7999.971386	11.433075	-0.063119	4.815357
314.549885	7999.984426	11.438080	-0.063133	4.815360
314.254663	8000.019056	11.443085	-0.063078	4.815372
314.177350	7999.996372	11.448090	-0.063063	4.815365
314.292951	8000.029266	11.453095	-0.063084	4.815375
314.280452	8000.021553	11.458099	-0.063082	4.815372
314.122603	7999.962258	11.463104	-0.063052	4.815356
314.207295	7999.993570	11.468109	-0.063068	4.815365
314.362437	7999.949088	11.473114	-0.063096	4.815351
314.201553	7999.948534	11.478119	-0.063066	4.815351
314.179818	7999.989839	11.483123	-0.063062	4.815364
314.290359	7999.926445	11.488128	-0.063082	4.815345
314.538878	7999.992542	11.493133	-0.063128	4.815363
314.262447	7999.950521	11.498138	-0.063076	4.815352
314.332289	7999.995483	11.503143	-0.063089	4.815365
314.434080	8000.036699	11.508147	-0.063108	4.815376
314.451008	8000.057267	11.513152	-0.063111	4.815382
314.550603	8000.059965	11.518157	-0.063129	4.815382
314.330562	7999.992155	11.523162	-0.063088	4.815364
314.188442	7999.989775	11.528167	-0.063061	4.815364
314.136046	8000.041260	11.533171	-0.063051	4.815379
314.233997	7999.959486	11.538176	-0.063069	4.815355
314.145206	7999.990058	11.543181	-0.063052	4.815364
314.264171	7999.952458	11.548186	-0.063074	4.815352
314.518296	8000.033614	11.553191	-0.063121	4.815375
314.326507	8000.030409	11.558195	-0.063085	4.815375
314.127510	7999.945846	11.563200	-0.063048	4.815351
314.260658	7999.980099	11.568205	-0.063072	4.815360
314.229748	7999.963530	11.573210	-0.063066	4.815356
314.191513	7999.958597	11.578215	-0.063059	4.815355
314.178551	7999.993634	11.583219	-0.063056	4.815365
314.287523	7999.951592	11.588224	-0.063076	4.815352
314.340992	7999.973835	11.593229	-0.063086	4.815358
314.423521	7999.912114	11.598234	-0.063101	4.815340
314.202769	7999.965082	11.603239	-0.063060	4.815356
314.423250	8000.025370	11.608243	-0.063101	4.815373
314.292107	7999.955829	11.613248	-0.063076	4.815353
314.405147	7999.986542	11.618253	-0.063097	4.815362
314.460952	7999.925447	11.623258	-0.063107	4.815344
314.274226	7999.935154	11.628263	-0.063072	4.815347
314.465887	7999.928689	11.633267	-0.063107	4.815345
314.450447	7999.908101	11.638272	-0.063104	4.815339
314.391831	7999.940242	11.643277	-0.063093	4.815348
314.466999	7999.900847	11.648282	-0.063107	4.815336
314.630273	7999.943083	11.653287	-0.063137	4.815348
314.541019	7999.956544	11.658291	-0.063120	4.815352
314.309968	7999.920621	11.663296	-0.063077	4.815343
314.334583	7999.938109	11.668301	-0.063081	4.815348
314.580557	7999.945373	11.673306	-0.063126	4.815349
314.451704	7999.962453	11.678311	-0.063102	4.815355
314.179891	8000.015643	11.683315	-0.063051	4.815371
314.425256	8000.017553	11.688320	-0.063097	4.815371
314.487504	8000.053838	11.693325	-0.063108	4.815381
314.294461	8000.012130	11.698330	-0.063072	4.815370
314.355153	7999.961805	11.703335	-0.063083	4.815355
314.343115	7999.964790	11.708339	-0.063080	4.815356
314.494474	7999.968346	11.713344	-0.063108	4.815356
314.465674	8000.067257	11.718349	-0.063103	4.815385
314.504911	8000.046506	11.723354	-0.063110	4.815379
314.297516	8000.018457	11.728359	-0.063071	4.815372
314.453586	7999.948335	11.733363	-0.063100	4.815350
314.711117	7999.939757	11.738368	-0.063147	4.815347
314.729965	7999.980667	11.743373	-0.063151	4.815359
314.613765	7999.930614	11.748378	-0.063129	4.815345
314.433937	7999.983192	11.753383	-0.063095	4.815361
314.455056	7999.951451	11.758387	-0.063099	4.815351
314.324916	7999.909719	11.763392	-0.063074	4.815340
314.514051	7999.966280	11.768397	-0.063109	4.815355
314.476070	8000.000902	11.773402	-0.063102	4.815366
314.700013	7999.985353	11.778407	-0.063143	4.815360
314.438844	7999.984204	11.783411	-0.063094	4.815361
314.550803	7999.957178	11.788416	-0.063115	4.815353
314.566178	7999.942445	11.793421	-0.063118	4.815348
314.458540	7999.923533	11.798426	-0.063097	4.815343
314.460656	7999.969509	11.803431	-0.063097	4.815357
314.573363	7999.968149	11.808435	-0.063118	4.815356
314.538201	7999.946164	11.813440	-0.063111	4.815350
314.512500	8000.028023	11.818445	-0.063106	4.815374
314.614429	8000.052139	11.823450	-0.063125	4.815380
314.734970	8000.028461	11.828455	-0.063147	4.815373
314.734245	8000.077597	11.833459	-0.063147	4.815387
314.657875	8000.002550	11.838464	-0.063132	4.815365
314.671918	8000.039104	11.843469	-0.063135	4.815376
314.499323	8000.030873	11.848474	-0.063102	4.815375
314.541816	8000.008038	11.853479	-0.063110	4.815368
314.678913	7999.969670	11.858483	-0.063135	4.815356
314.535060	7999.960847	11.863488	-0.063108	4.815354
314.640649	8000.061987	11.868493	-0.063128	4.815383
314.635950	7999.959268	11.873498	-0.063126	4.815353
314.524799	7999.978780	11.878503	-0.063106	4.815359
314.449653	8000.018130	11.883507	-0.063091	4.815371
314.326607	7999.985067	11.888512	-0.063068	4.815362
314.561920	8000.029567	11.893517	-0.063112	4.815374
314.399142	8000.016154	11.898522	-0.063081	4.815371
314.592633	8000.048202	11.903527	-0.063117	4.815379
314.577268	8000.043649	11.908531	-0.063114	4.815378
314.477336	7999.934005	11.913536	-0.063095	4.815346
314.639731	8000.010433	11.918541	-0.063125	4.815368
314.491747	8000.021851	11.923546	-0.063097	4.815372
314.503473	7999.986748	11.928551	-0.063099	4.815362
314.483853	8000.030226	11.933555	-0.063095	4.815375
314.474375	7999.945600	11.938560	-0.063093	4.815350
314.686245	8000.033537	11.943565	-0.063132	4.815375
314.634485	8000.008070	11.948570	-0.063122	4.815367
314.660256	8000.031991	11.953575	-0.063127	4.815374
314.584583	8000.027506	11.958579	-0.063113	4.815373
314.541576	8000.008598	11.963584	-0.063104	4.815368
314.435177	8000.002534	11.968589	-0.063084	4.815367
314.500847	7999.944809	11.973594	-0.063096	4.815350
314.575015	8000.011221	11.978599	-0.063110	4.815369
314.590888	8000.026427	11.983603	-0.063112	4.815373
314.658458	8000.009353	11.988608	-0.063125	4.815368
314.787490	8000.052090	11.993613	-0.063149	4.815380
314.710413	8000.006962	11.998618	-0.063134	4.815367
314.718700	7999.988904	12.003623	-0.063135	4.815361
314.592781	7999.976103	12.008627	-0.063111	4.815358
314.647765	7999.939579	12.013632	-0.063121	4.815347
314.766700	7999.985356	12.018637	-0.063143	4.815360
314.744958	7999.983903	12.023642	-0.063139	4.815360
314.634417	7999.948909	12.028647	-0.063118	4.815350
314.609842	8000.023304	12.033651	-0.063113	4.815372
314.417970	8000.013685	12.038656	-0.063077	4.815370
314.728636	8000.048746	12.043661	-0.063135	4.815379
314.661390	8000.031573	12.048666	-0.063122	4.815374
314.669800	7999.970760	12.053671	-0.063124	4.815356
314.885192	8000.077998	12.058675	-0.063163	4.815387
314.798089	7999.978187	12.063680	-0.063147	4.815358
314.742781	8000.000763	12.068685	-0.063136	4.815365
314.712840	8000.014140	12.073690	-0.063131	4.815369
314.850135	8000.031360	12.078695	-0.063156	4.815373
314.827195	8000.027749	12.083699	-0.063151	4.815372
314.634844	7999.975364	12.088704	-0.063115	4.815358
314.877080	8000.055255	12.093709	-0.063160	4.815380
314.763391	7999.983864	12.098714	-0.063139	4.815360
314.683249	7999.983581	12.103719	-0.063123	4.815360
314.614005	8000.020891	12.108723	-0.063110	4.815371
314.408507	7999.967219	12.113728	-0.063072	4.815357
314.452478	7999.963649	12.118733	-0.063080	4.815355
314.475607	7999.964010	12.123738	-0.063084	4.815355
314.663574	7999.987415	12.128743	-0.063118	4.815361
314.656005	7999.971232	12.133747	-0.063117	4.815357
314.358418	7999.910689	12.138752	-0.063061	4.815340
314.624534	8000.016629	12.143757	-0.063110	4.815370
314.600969	8000.019421	12.148762	-0.063106	4.815371
314.581974	7999.981671	12.153767	-0.063102	4.815360
314.428215	8000.033612	12.158771	-0.063073	4.815376
314.759105	7999.994184	12.163776	-0.063134	4.815363
314.636348	8000.065881	12.168781	-0.063111	4.815385
314.639650	8000.049878	12.173786	-0.063112	4.815380
314.672794	8000.040785	12.178791	-0.063118	4.815377
314.835070	8000.061626	12.183795	-0.063148	4.815382
314.651944	7999.993360	12.188800	-0.063113	4.815363
314.668218	7999.961539	12.193805	-0.063116	4.815354
314.630387	7999.968371	12.198810	-0.063109	4.815356
314.583709	7999.987883	12.203815	-0.063100	4.815362
314.820219	8000.027059	12.208819	-0.063144	4.815372
314.843491	7999.964354	12.213824	-0.063148	4.815354
314.775062	8000.052987	12.218829	-0.063135	4.815380
314.807200	8000.002188	12.223834	-0.063140	4.815365
314.815098	7999.968090	12.228839	-0.063142	4.815355
314.798655	8000.009483	12.233843	-0.063138	4.815367
314.656482	7999.969689	12.238848	-0.063111	4.815356
314.790102	7999.988985	12.243853	-0.063136	4.815361
314.865970	7999.981669	12.248858	-0.063150	4.815359
314.848509	7999.992046	12.253863	-0.063146	4.815362
314.829959	8000.006681	12.258867	-0.063143	4.815366
314.794385	7999.990033	12.263872	-0.063136	4.815362
314.827267	8000.033313	12.268877	-0.063142	4.815374
314.682266	8000.030885	12.273882	-0.063115	4.815374
314.660872	8000.004852	12.278887	-0.063110	4.815367
314.864014	8000.026372	12.283891	-0.063148	4.815372
314.677262	7999.938804	12.288896	-0.063113	4.815347
314.679857	7999.997616	12.293901	-0.063113	4.815365
314.717346	7999.967215	12.298906	-0.063120	4.815355
314.647836	7999.960695	12.303911	-0.063107	4.815354
314.839744	7999.995924	12.308915	-0.063142	4.815363
314.817493	7999.982704	12.313920	-0.063138	4.815360
314.921848	8000.039997	12.318925	-0.063157	4.815376
314.853262	7999.949045	12.323930	-0.063144	4.815350
314.820005	7999.944195	12.328935	-0.063137	4.815348
314.867310	7999.983439	12.333939	-0.063146	4.815360
314.763392	7999.949623	12.338944	-0.063126	4.815350
314.788011	8000.010938	12.343949	-0.063131	4.815368
314.795815	7999.973632	12.348954	-0.063132	4.815357
314.851204	7999.956356	12.353959	-0.063142	4.815352
314.998780	7999.992987	12.358963	-0.063169	4.815362
314.764915	7999.945258	12.363968	-0.063125	4.815349
314.956216	7999.996511	12.368973	-0.063161	4.815363
314.713007	7999.968936	12.373978	-0.063115	4.815356
314.814232	8000.014419	12.378983	-0.063134	4.815369
314.829252	8000.071299	12.383987	-0.063136	4.815385
314.647294	7999.976329	12.388992	-0.063102	4.815359
314.625047	7999.969523	12.393997	-0.063098	4.815357
314.618387	7999.918081	12.399002	-0.063096	4.815342
314.750450	7999.963006	12.404007	-0.063120	4.815354
314.827814	8000.007024	12.409011	-0.063135	4.815367
314.796888	7999.957317	12.414016	-0.063129	4.815352
314.910580	7999.996593	12.419021	-0.063150	4.815363
314.839551	7999.997529	12.424026	-0.063136	4.815364
314.900059	7999.969649	12.429031	-0.063147	4.815355
315.031561	8000.040220	12.434035	-0.063171	4.815375
314.816763	7999.956463	12.439040	-0.063131	4.815352
315.076035	7999.944707	12.444045	-0.063179	4.815347
314.896550	7999.973774	12.449050	-0.063145	4.815357
314.907090	7999.963237	12.454055	-0.063147	4.815354
314.892919	7999.946945	12.459059	-0.063144	4.815349
314.544690	7999.909077	12.464064	-0.063079	4.815340
314.864809	7999.960329	12.469069	-0.063138	4.815353
314.630435	7999.953211	12.474074	-0.063094	4.815352
314.661521	7999.970806	12.479079	-0.063100	4.815357
314.801402	8000.005172	12.484083	-0.063126	4.815366
314.943592	7999.956199	12.489088	-0.063152	4.815351
314.804432	7999.961350	12.494093	-0.063126	4.815354
314.885625	7999.951984	12.499098	-0.063141	4.815350
314.967963	7999.967224	12.504103	-0.063156	4.815355
314.954885	8000.020431	12.509107	-0.063153	4.815370
314.640464	7999.956400	12.514112	-0.063094	4.815353
314.850811	7999.978038	12.519117	-0.063133	4.815358
314.678153	7999.958048	12.524122	-0.063101	4.815353
314.707955	7999.953175	12.529127	-0.063106	4.815352
314.791300	7999.965224	12.534131	-0.063121	4.815355
314.696873	7999.951876	12.539136	-0.063104	4.815351
314.708838	7999.968086	12.544141	-0.063105	4.815356
314.639040	7999.939113	12.549146	-0.063092	4.815348
314.831977	7999.972220	12.554151	-0.063128	4.815357
314.888126	8000.007335	12.559155	-0.063138	4.815367
314.847500	7999.967087	12.564160	-0.063130	4.815355
315.149281	7999.980622	12.569165	-0.063186	4.815358
314.933915	8000.021922	12.574170	-0.063146	4.815371
314.862971	7999.975826	12.579175	-0.063132	4.815358
314.993470	8000.026071	12.584179	-0.063156	4.815372
314.905547	7999.958315	12.589184	-0.063140	4.815352
314.936652	8000.007979	12.594189	-0.063145	4.815367
314.721806	7999.983013	12.599194	-0.063105	4.815360
314.935611	7999.959813	12.604199	-0.063145	4.815353
314.849870	8000.009677	12.609203	-0.063128	4.815368
314.776789	7999.960339	12.614208	-0.063115	4.815354
314.869879	8000.017445	12.619213	-0.063132	4.815370
314.832052	7999.978313	12.624218	-0.063124	4.815359
314.911389	7999.997778	12.629223	-0.063139	4.815364
315.043082	7999.968941	12.634227	-0.063163	4.815355
314.806174	7999.959643	12.639232	-0.063119	4.815353
314.875706	8000.011014	12.644237	-0.063131	4.815368
314.775579	7999.986882	12.649242	-0.063113	4.815361
315.013211	7999.959802	12.654247	-0.063156	4.815352
314.933380	7999.983040	12.659251	-0.063141	4.815360
314.952247	7999.981192	12.664256	-0.063145	4.815359
315.060168	7999.992580	12.669261	-0.063164	4.815362
315.028407	7999.971720	12.674266	-0.063158	4.815356
314.965529	7999.949275	12.679271	-0.063146	4.815350
314.909263	8000.006042	12.684275	-0.063136	4.815366
315.033770	7999.971740	12.689280	-0.063159	4.815356
314.823718	8000.021679	12.694285	-0.063119	4.815371
314.898901	8000.022904	12.699290	-0.063133	4.815371
314.997226	7999.983892	12.704295	-0.063151	4.815360
315.032586	8000.075316	12.709299	-0.063157	4.815386
314.754530	8000.018302	12.714304	-0.063105	4.815371
314.935750	7999.993493	12.719309	-0.063139	4.815363
314.979624	7999.995267	12.724314	-0.063147	4.815363
314.854064	7999.969644	12.729319	-0.063123	4.815356
314.870243	7999.964545	12.734323	-0.063126	4.815355
315.063936	7999.953839	12.739328	-0.063162	4.815350
314.989266	8000.007093	12.744333	-0.063147	4.815366
314.956791	7999.980877	12.749338	-0.063141	4.815359
314.992180	8000.026336	12.754343	-0.063147	4.815372
315.043677	8000.013271	12.759347	-0.063157	4.815368
314.986573	7999.920372	12.764352	-0.063146	4.815341
315.126596	7999.951534	12.769357	-0.063172	4.815350
315.024142	7999.941259	12.774362	-0.063152	4.815347
314.837648	7999.929591	12.779367	-0.063117	4.815345
314.835932	7999.970159	12.784371	-0.063117	4.815356
314.810515	7999.963301	12.789376	-0.063112	4.815355
314.794128	7999.973695	12.794381	-0.063108	4.815358
314.981324	7999.962882	12.799386	-0.063143	4.815354
315.018076	7999.955986	12.804391	-0.063150	4.815351
315.241974	7999.975712	12.809395	-0.063191	4.815356
314.999602	7999.948151	12.814400	-0.063146	4.815349
314.974567	8000.026814	12.819405	-0.063141	4.815372
315.201758	7999.973907	12.824410	-0.063183	4.815356
315.113525	7999.957454	12.829415	-0.063166	4.815351
315.082322	7999.994327	12.834419	-0.063160	4.815362
315.041894	7999.934841	12.839424	-0.063152	4.815345
315.138087	7999.958862	12.844429	-0.063170	4.815352
315.041886	7999.935864	12.849434	-0.063152	4.815345
314.977353	7999.966839	12.854439	-0.063139	4.815355
314.957977	7999.993218	12.859443	-0.063136	4.815363
314.771591	7999.973000	12.864448	-0.063101	4.815358
315.009261	7999.987609	12.869453	-0.063145	4.815361
314.944224	7999.923440	12.874458	-0.063132	4.815342
315.029215	7999.906655	12.879463	-0.063148	4.815337
315.030395	7999.987891	12.884467	-0.063148	4.815361
314.884005	7999.940544	12.889472	-0.063120	4.815348
315.022034	7999.995188	12.894477	-0.063146	4.815363
315.007926	8000.043034	12.899482	-0.063143	4.815377
314.994923	7999.985072	12.904487	-0.063140	4.815360
315.065884	8000.054639	12.909491	-0.063153	4.815380
314.893592	7999.989759	12.914496	-0.063121	4.815362
315.181785	8000.015896	12.919501	-0.063174	4.815368
315.224719	8000.031551	12.924506	-0.063182	4.815373
315.120749	7999.960321	12.929511	-0.063162	4.815352
315.127988	7999.972177	12.934515	-0.063163	4.815356
315.037730	7999.935381	12.939520	-0.063146	4.815345
315.009173	7999.949850	12.944525	-0.063141	4.815350
314.849673	7999.957870	12.949530	-0.063111	4.815353
315.139456	7999.971206	12.954535	-0.063165	4.815355
315.259349	8000.027689	12.959539	-0.063187	4.815371
315.183994	7999.977244	12.964544	-0.063172	4.815357
315.081880	7999.966975	12.969549	-0.063153	4.815355
315.176291	7999.946071	12.974554	-0.063170	4.815348
315.098042	7999.966128	12.979559	-0.063155	4.815354
315.051518	7999.979230	12.984563	-0.063147	4.815358
315.100650	7999.923368	12.989568	-0.063155	4.815342
315.272644	7999.981783	12.994573	-0.063187	4.815358
315.168304	7999.978960	12.999578	-0.063168	4.815358
315.009754	7999.924998	13.004583	-0.063138	4.815343
315.205132	7999.942112	13.009587	-0.063174	4.815347
315.094066	7999.952005	13.014592	-0.063153	4.815350
315.003138	7999.971852	13.019597	-0.063136	4.815356
315.061233	8000.049757	13.024602	-0.063146	4.815379
315.013945	7999.966641	13.029607	-0.063137	4.815355
315.192313	8000.023024	13.034611	-0.063170	4.815370
314.996153	8000.018678	13.039616	-0.063133	4.815370
315.006869	7999.980351	13.044621	-0.063135	4.815359
315.034111	8000.003227	13.049626	-0.063140	4.815365
314.911290	7999.928479	13.054631	-0.063117	4.815344
315.092967	7999.960331	13.059635	-0.063150	4.815353
315.023079	7999.919598	13.064640	-0.063137	4.815341
314.955822	7999.972975	13.069645	-0.063124	4.815357
315.311553	7999.999164	13.074650	-0.063190	4.815363
315.309867	7999.963838	13.079655	-0.063190	4.815353
315.032620	7999.997697	13.084659	-0.063138	4.815364
315.021963	7999.942981	13.089664	-0.063136	4.815348
315.139270	7999.974835	13.094669	-0.063157	4.815357
315.206395	8000.025097	13.099674	-0.063170	4.815371
314.993367	7999.952058	13.104679	-0.063130	4.815351
315.091311	7999.999625	13.109683	-0.063148	4.815364
315.076062	7999.924523	13.114688	-0.063144	4.815342
314.878146	7999.950078	13.119693	-0.063107	4.815351
315.105596	8000.003000	13.124698	-0.063149	4.815365
315.052481	7999.975372	13.129703	-0.063139	4.815357
315.039594	8000.033927	13.134707	-0.063137	4.815375
315.024274	7999.964169	13.139712	-0.063134	4.815354
315.142831	7999.983215	13.144717	-0.063155	4.815359
315.066745	8000.013998	13.149722	-0.063141	4.815369
315.075878	8000.008782	13.154727	-0.063142	4.815367
315.143497	8000.045156	13.159731	-0.063155	4.815377
315.073130	8000.006553	13.164736	-0.063141	4.815366
315.000387	7999.973255	13.169741	-0.063128	4.815357
315.023804	7999.988585	13.174746	-0.063132	4.815361
315.188786	7999.954956	13.179751	-0.063162	4.815351
315.085751	7999.998119	13.184755	-0.063143	4.815364
315.017465	7999.911448	13.189760	-0.063130	4.815339
315.131744	7999.984939	13.194765	-0.063151	4.815360
315.124605	7999.950592	13.199770	-0.063149	4.815350
314.810406	7999.943219	13.204775	-0.063090	4.815349
315.072596	8000.033060	13.209779	-0.063139	4.815374
315.094427	8000.037675	13.214784	-0.063143	4.815375
315.051499	8000.003803	13.219789	-0.063134	4.815366
315.123429	7999.953664	13.224794	-0.063148	4.815351
315.212376	7999.921980	13.229799	-0.063164	4.815341
315.334870	7999.953919	13.234803	-0.063186	4.815350
315.207888	7999.975306	13.239808	-0.063163	4.815357
315.162940	7999.979882	13.244813	-0.063154	4.815358
315.095510	8000.030050	13.249818	-0.063141	4.815373
315.072036	7999.954812	13.254823	-0.063136	4.815351
315.161364	7999.986201	13.259827	-0.063153	4.815360
315.342651	7999.919704	13.264832	-0.063186	4.815340
315.097204	7999.962643	13.269837	-0.063140	4.815354
314.987788	7999.987528	13.274842	-0.063120	4.815361
315.247209	7999.970430	13.279847	-0.063168	4.815355
315.170001	8000.082434	13.284851	-0.063153	4.815388
315.022346	7999.999791	13.289856	-0.063125	4.815365
315.311946	7999.975711	13.294861	-0.063179	4.815356
315.297000	7999.993612	13.299866	-0.063176	4.815362
315.172046	7999.959448	13.304871	-0.063152	4.815352
315.295113	7999.984983	13.309875	-0.063175	4.815359
315.370811	7999.958424	13.314880	-0.063189	4.815351
315.365195	7999.967928	13.319885	-0.063188	4.815354
315.271622	7999.995214	13.324890	-0.063170	4.815362
315.234147	7999.907985	13.329895	-0.063163	4.815337
315.284932	7999.940873	13.334899	-0.063172	4.815346
315.223955	7999.914184	13.339904	-0.063160	4.815339
315.268772	7999.945903	13.344909	-0.063168	4.815348
315.195991	7999.960707	13.349914	-0.063155	4.815353
315.061318	7999.933864	13.354919	-0.063129	4.815345
315.101446	7999.972989	13.359923	-0.063137	4.815357
315.326144	7999.951039	13.364928	-0.063178	4.815349
315.254658	7999.962657	13.369933	-0.063165	4.815353
315.148544	7999.950184	13.374938	-0.063145	4.815350
315.104014	7999.917355	13.379943	-0.063136	4.815340
315.151357	7999.945909	13.384947	-0.063145	4.815349
315.119844	7999.951777	13.389952	-0.063138	4.815350
315.212215	7999.952218	13.394957	-0.063155	4.815350
315.283303	7999.962994	13.399962	-0.063168	4.815353
315.085002	7999.934027	13.404967	-0.063131	4.815345
315.177467	7999.990054	13.409971	-0.063148	4.815361
315.053599	7999.952701	13.414976	-0.063125	4.815351
315.208090	7999.922104	13.419981	-0.063153	4.815341
315.086314	8000.013058	13.424986	-0.063130	4.815369
315.142500	7999.985106	13.429991	-0.063141	4.815360
315.231593	8000.001526	13.434995	-0.063157	4.815365
315.051622	7999.997449	13.440000	-0.063123	4.815364
314.942806	7999.956070	13.445005	-0.063103	4.815353
315.192481	7999.968740	13.450010	-0.063149	4.815355
315.143300	7999.917661	13.455015	-0.063139	4.815340
315.142205	7999.997790	13.460019	-0.063139	4.815364
315.025020	7999.937032	13.465024	-0.063117	4.815347
315.324489	7999.990079	13.470029	-0.063172	4.815361
315.264091	7999.962331	13.475034	-0.063161	4.815353
315.201561	7999.952719	13.480039	-0.063149	4.815350
315.401811	7999.969914	13.485043	-0.063186	4.815355
315.139058	7999.964463	13.490048	-0.063137	4.815354
315.167749	7999.970261	13.495053	-0.063142	4.815356
315.150539	7999.976366	13.500058	-0.063138	4.815358
315.162108	7999.986155	13.505063	-0.063140	4.815360
315.272020	7999.997576	13.510067	-0.063161	4.815363
315.283712	7999.957128	13.515072	-0.063162	4.815351
315.323103	7999.967379	13.520077	-0.063170	4.815354
315.178546	7999.979923	13.525082	-0.063142	4.815359
314.996135	7999.939461	13.530087	-0.063108	4.815348
315.212968	7999.979379	13.535091	-0.063148	4.815358
315.148005	7999.968657	13.540096	-0.063136	4.815355
314.993557	8000.000278	13.545101	-0.063107	4.815365
315.013307	7999.978135	13.550106	-0.063110	4.815359
315.073112	7999.926727	13.555111	-0.063121	4.815344
315.294675	7999.977412	13.560115	-0.063162	4.815357
315.146148	7999.956753	13.565120	-0.063134	4.815352
315.343617	7999.974972	13.570125	-0.063171	4.815356
315.247933	7999.991533	13.575130	-0.063153	4.815362
315.252346	7999.964860	13.580135	-0.063153	4.815354
315.366809	7999.971012	13.585139	-0.063174	4.815355
315.408156	7999.946020	13.590144	-0.063182	4.815348
315.298913	7999.974115	13.595149	-0.063161	4.815356
315.366682	7999.975216	13.600154	-0.063174	4.815356
315.312022	7999.917633	13.605159	-0.063163	4.815340
315.280321	7999.954497	13.610163	-0.063157	4.815351
315.295116	7999.940823	13.615168	-0.063159	4.815347
315.362324	7999.945122	13.620173	-0.063172	4.815348
315.341543	7999.968271	13.625178	-0.063168	4.815355
315.184184	7999.933569	13.630183	-0.063138	4.815345
315.285582	7999.959814	13.635187	-0.063157	4.815352
315.145726	7999.916851	13.640192	-0.063130	4.815340
315.112690	7999.946210	13.645197	-0.063124	4.815349
315.236183	7999.954649	13.650202	-0.063147	4.815351
315.237101	7999.998468	13.655207	-0.063147	4.815364
315.279526	8000.009838	13.660211	-0.063154	4.815367
315.234290	7999.954549	13.665216	-0.063146	4.815351
315.353213	7999.966119	13.670221	-0.063167	4.815354
315.280511	7999.906099	13.675226	-0.063154	4.815337
315.238287	7999.940650	13.680231	-0.063145	4.815347
315.342768	7999.969084	13.685235	-0.063165	4.815355
315.411705	7999.935999	13.690240	-0.063177	4.815345
315.469279	7999.952965	13.695245	-0.063188	4.815350
315.514833	8000.021041	13.700250	-0.063196	4.815369
315.327000	7999.950558	13.705255	-0.063161	4.815350
315.360649	7999.991713	13.710259	-0.063167	4.815361
315.339813	7999.971035	13.715264	-0.063163	4.815355
315.428561	7999.958588	13.720269	-0.063179	4.815351
315.479261	8000.031026	13.725274	-0.063188	4.815372
315.360639	7999.984139	13.730279	-0.063166	4.815359
315.655070	8000.039242	13.735283	-0.063220	4.815374
315.557930	7999.962780	13.740288	-0.063202	4.815352
315.611272	7999.961505	13.745293	-0.063212	4.815351
315.576087	7999.983346	13.750298	-0.063205	4.815358
315.590920	7999.944018	13.755303	-0.063207	4.815346
315.655081	7999.965369	13.760307	-0.063219	4.815352
315.530180	7999.953653	13.765312	-0.063195	4.815350
315.573211	7999.971447	13.770317	-0.063203	4.815355
315.354615	7999.940005	13.775322	-0.063162	4.815346
315.324595	7999.953380	13.780327	-0.063156	4.815350
315.248431	7999.939267	13.785331	-0.063142	4.815347
315.211629	7999.929013	13.790336	-0.063135	4.815344
315.427859	7999.938990	13.795341	-0.063175	4.815346
315.566386	7999.986161	13.800346	-0.063200	4.815359
315.360675	7999.933554	13.805351	-0.063162	4.815345
315.315543	7999.968057	13.810355	-0.063153	4.815355
315.236186	7999.922891	13.815360	-0.063138	4.815342
315.324703	7999.916854	13.820365	-0.063154	4.815340
315.455127	7999.973511	13.825370	-0.063178	4.815356
315.287188	7999.937565	13.830375	-0.063147	4.815346
315.356798	7999.973972	13.835379	-0.063160	4.815356
315.349558	7999.953519	13.840384	-0.063158	4.815350
315.337363	7999.941535	13.845389	-0.063155	4.815347
315.320190	7999.974364	13.850394	-0.063152	4.815357
315.338076	7999.968224	13.855399	-0.063155	4.815355
315.445208	7999.973185	13.860403	-0.063175	4.815356
315.441044	7999.986990	13.865408	-0.063174	4.815360
315.374008	7999.962338	13.870413	-0.063161	4.815353
315.390011	7999.955098	13.875418	-0.063164	4.815351
315.516951	7999.929388	13.880423	-0.063187	4.815343
315.416383	7999.956558	13.885427	-0.063168	4.815351
315.495551	7999.979228	13.890432	-0.063183	4.815357
315.466227	8000.010786	13.895437	-0.063177	4.815367
315.398731	8000.050263	13.900442	-0.063164	4.815379
315.441418	7999.964364	13.905447	-0.063172	4.815353
315.601354	8000.032201	13.910451	-0.063201	4.815372
315.520269	7999.942110	13.915456	-0.063186	4.815346
315.657433	7999.929397	13.920461	-0.063211	4.815342
315.549107	7999.994920	13.925466	-0.063191	4.815362
315.338044	7999.966810	13.930471	-0.063151	4.815355
315.460344	8000.024401	13.935475	-0.063174	4.815371
315.502728	8000.002633	13.940480	-0.063181	4.815364
315.412212	8000.009660	13.945485	-0.063164	4.815367
315.560588	8000.056995	13.950490	-0.063192	4.815380
315.468414	7999.968858	13.955495	-0.063174	4.815355
315.628066	8000.013173	13.960499	-0.063204	4.815367
315.559649	8000.016290	13.965504	-0.063191	4.815368
315.556671	7999.990563	13.970509	-0.063190	4.815360
315.544461	7999.982855	13.975514	-0.063187	4.815358
315.678414	7999.989330	13.980519	-0.063212	4.815360
315.681585	8000.025704	13.985523	-0.063212	4.815370
315.790569	7999.972973	13.990528	-0.063232	4.815354
315.768573	7999.976861	13.995533	-0.063228	4.815355
315.723100	7999.973946	14.000538	-0.063219	4.815355
315.712690	7999.923509	14.005543	-0.063217	4.815340
315.760242	7999.981999	14.010547	-0.063226	4.815357
315.562173	7999.954103	14.015552	-0.063188	4.815350
315.468577	7999.950390	14.020557	-0.063171	4.815349
315.652245	8000.012206	14.025562	-0.063205	4.815366
315.636865	7999.944584	14.030567	-0.063202	4.815347
315.764501	7999.966989	14.035571	-0.063225	4.815353
315.685623	7999.934658	14.040576	-0.063210	4.815344
315.736125	7999.973955	14.045581	-0.063219	4.815355
315.682239	7999.994417	14.050586	-0.063209	4.815361
315.559033	7999.925006	14.055591	-0.063186	4.815341
315.650431	7999.971395	14.060595	-0.063203	4.815355
315.596056	7999.997193	14.065600	-0.063192	4.815362
315.677492	7999.955764	14.070605	-0.063207	4.815350
315.717806	7999.986340	14.075610	-0.063214	4.815359
315.697273	7999.938943	14.080615	-0.063210	4.815345
315.752082	7999.945174	14.085619	-0.063220	4.815346
315.697006	7999.961340	14.090624	-0.063210	4.815351
315.524172	7999.954174	14.095629	-0.063177	4.815350
315.493613	7999.964333	14.100634	-0.063171	4.815353
315.585558	7999.914527	14.105639	-0.063188	4.815338
315.831072	7999.948507	14.110643	-0.063234	4.815347
315.708779	7999.925076	14.115648	-0.063211	4.815341
315.787764	7999.955226	14.120653	-0.063225	4.815349
315.850922	8000.008629	14.125658	-0.063237	4.815365
315.775349	7999.937870	14.130663	-0.063222	4.815344
315.558314	7999.947074	14.135667	-0.063182	4.815348
315.857745	7999.973398	14.140672	-0.063237	4.815354
315.919514	7999.959435	14.145677	-0.063248	4.815350
315.849121	7999.973209	14.150682	-0.063235	4.815354
315.557657	7999.967281	14.155687	-0.063180	4.815354
315.918830	8000.010664	14.160691	-0.063247	4.815365
315.801398	8000.005485	14.165696	-0.063225	4.815364
315.782422	7999.969872	14.170701	-0.063222	4.815354
315.898999	8000.053024	14.175706	-0.063243	4.815377
315.579175	7999.946144	14.180711	-0.063183	4.815348
315.680618	7999.974528	14.185715	-0.063202	4.815355
315.728466	7999.978505	14.190720	-0.063210	4.815356
315.687331	7999.986351	14.195725	-0.063203	4.815359
315.595026	7999.995486	14.200730	-0.063185	4.815362
315.656773	7999.995419	14.205735	-0.063196	4.815362
315.803615	7999.979660	14.210739	-0.063223	4.815356
315.693837	8000.018436	14.215744	-0.063203	4.815368
315.602040	7999.971994	14.220749	-0.063185	4.815355
315.819655	8000.005512	14.225754	-0.063226	4.815364
315.683841	7999.990408	14.230759	-0.063200	4.815360
315.693898	8000.013000	14.235763	-0.063202	4.815367
315.677085	8000.040491	14.240768	-0.063198	4.815375
315.972118	7999.990847	14.245773	-0.063253	4.815359
315.968598	8000.022834	14.250778	-0.063252	4.815368
315.678182	7999.972027	14.255783	-0.063198	4.815355
315.876474	7999.994536	14.260787	-0.063234	4.815360
315.740634	7999.986914	14.265792	-0.063209	4.815359
315.864653	7999.096399	14.270797	-0.063231	4.815098
315.797436	7996.002180	14.275802	-0.063216	4.814195
315.523194	7990.521544	14.280807	-0.063161	4.812595
315.407080	7983.889871	14.285811	-0.063135	4.810657
315.690619	7976.615115	14.290816	-0.063183	4.808528
315.614689	7968.973966	14.295821	-0.063164	4.806293
315.514544	7961.230453	14.300826	-0.063140	4.804027
315.525133	7953.361244	14.305831	-0.063136	4.801723
315.620575	7945.380986	14.310835	-0.063149	4.799385
315.301396	7937.447323	14.315840	-0.063084	4.797061
315.259364	7929.365301	14.320845	-0.063070	4.794691
315.385621	7921.405728	14.325850	-0.063088	4.792355
315.322458	7913.328163	14.330855	-0.063071	4.789984
315.304231	7905.450822	14.335859	-0.063062	4.787670
315.316966	7897.372727	14.340864	-0.063059	4.785297
315.410411	7889.416557	14.345869	-0.063071	4.782958
315.324822	7881.428899	14.350874	-0.063050	4.780609
315.119268	7873.389491	14.355879	-0.063006	4.778244
315.271049	7865.412983	14.360883	-0.063029	4.775895
315.190536	7857.389616	14.365888	-0.063008	4.773532
315.140498	7849.327233	14.370893	-0.062993	4.771156
315.389187	7841.388088	14.375898	-0.063034	4.768814
315.260516	7833.388767	14.380903	-0.063005	4.766455
315.239568	7825.368359	14.385907	-0.062996	4.764088
315.016273	7817.442507	14.390912	-0.062949	4.761748
315.085850	7809.344553	14.395917	-0.062956	4.759355
315.071646	7801.448183	14.400922	-0.062948	4.757021
315.093729	7793.364037	14.405927	-0.062946	4.754630
315.022208	7785.324032	14.410931	-0.062928	4.752252
314.881065	7777.257787	14.415936	-0.062896	4.749864
314.746756	7769.327465	14.420941	-0.062865	4.747516
314.696645	7761.375704	14.425946	-0.062851	4.745160
314.795057	7753.340012	14.430951	-0.062864	4.742777
314.742969	7745.339381	14.435955	-0.062848	4.740404
314.819124	7737.330426	14.440960	-0.062857	4.738027
314.785015	7729.267599	14.445965	-0.062845	4.735633
314.761412	7721.317191	14.450970	-0.062835	4.733271
314.578725	7713.271574	14.455975	-0.062796	4.730880
314.392526	7705.316136	14.460979	-0.062756	4.728515
314.503513	7697.325548	14.465984	-0.062771	4.726137
314.381381	7689.284409	14.470989	-0.062743	4.723744
314.303043	7681.328484	14.475994	-0.062723	4.721375
314.264744	7673.295238	14.480999	-0.062710	4.718981
314.329376	7665.315124	14.486003	-0.062717	4.716602
314.251668	7657.321099	14.491008	-0.062697	4.714218
314.305479	7649.259011	14.496013	-0.062701	4.711811
314.347204	7641.274107	14.501018	-0.062703	4.709427
314.155937	7633.314429	14.506023	-0.062662	4.707050
314.209439	7625.265667	14.511027	-0.062667	4.704644
314.293647	7617.321434	14.516032	-0.062677	4.702268
314.363761	7609.256950	14.521037	-0.062685	4.699855
314.188131	7601.373182	14.526042	-0.062647	4.697495
314.013565	7593.290242	14.531047	-0.062609	4.695075
314.079621	7585.284992	14.536051	-0.062615	4.692676
313.811667	7577.236931	14.541056	-0.062560	4.690264
313.757443	7569.277682	14.546061	-0.062544	4.687876
314.043291	7561.305827	14.551066	-0.062592	4.685483
313.601929	7553.288008	14.556071	-0.062505	4.683077
313.712261	7545.290036	14.561075	-0.062520	4.680674
314.043291	7537.328478	14.566080	-0.062576	4.678280
313.816753	7529.266272	14.571085	-0.062528	4.675856
313.762574	7521.196757	14.576090	-0.062512	4.673428
313.726795	7513.147106	14.581095	-0.062500	4.671004
313.811258	7505.204796	14.586099	-0.062511	4.668612
313.711788	7497.185973	14.591104	-0.062487	4.666196
313.869216	7489.242827	14.596109	-0.062510	4.663800
313.910507	7481.284619	14.601114	-0.062513	4.661400
313.618513	7473.218576	14.606119	-0.062453	4.658965
313.536277	7465.201045	14.611123	-0.062432	4.656544
313.694321	7457.239170	14.616128	-0.062456	4.654138
313.612094	7449.211403	14.621133	-0.062435	4.651712
313.504718	7441.190884	14.626138	-0.062410	4.649286
313.573450	7433.236991	14.631143	-0.062417	4.646879
313.648822	7425.174856	14.636147	-0.062426	4.644438
313.561108	7417.262839	14.641152	-0.062404	4.642041
313.370473	7409.189951	14.646157	-0.062363	4.639594
313.595409	7401.315771	14.651162	-0.062399	4.637206
313.505968	7393.178538	14.656167	-0.062377	4.634737
313.210873	7385.190303	14.661171	-0.062317	4.632312
313.174187	7377.167716	14.666176	-0.062304	4.629876
313.072095	7369.142100	14.671181	-0.062280	4.627437
313.138717	7361.184597	14.676186	-0.062287	4.625017
313.057208	7353.206480	14.681191	-0.062266	4.622590
312.977746	7345.159789	14.686195	-0.062246	4.620141
312.937152	7337.198393	14.691200	-0.062233	4.617716
312.811258	7329.176639	14.696205	-0.062204	4.615272
313.131740	7321.167451	14.701210	-0.062258	4.612831
312.869320	7313.087715	14.706215	-0.062204	4.610366
312.743766	7305.170897	14.711219	-0.062175	4.607950
312.958818	7297.148772	14.716224	-0.062210	4.605500
312.986030	7289.186124	14.721229	-0.062209	4.603068
312.814940	7281.210487	14.726234	-0.062172	4.600630
312.672910	7273.188098	14.731239	-0.062140	4.598176
312.942716	7265.173639	14.736243	-0.062185	4.595724
312.768664	7257.116068	14.741248	-0.062147	4.593257
312.551082	7249.092520	14.746253	-0.062101	4.590799
312.695153	7241.125671	14.751258	-0.062122	4.588357
312.659374	7233.068716	14.756263	-0.062110	4.585886
312.518195	7225.109943	14.761267	-0.062078	4.583444
312.432020	7217.140094	14.766272	-0.062057	4.580998
312.391985	7209.138861	14.771277	-0.062044	4.578540
312.505269	7201.150668	14.776282	-0.062059	4.576085
312.442662	7193.138822	14.781287	-0.062042	4.573622
312.573475	7185.074921	14.786291	-0.062061	4.571141
312.438720	7177.107498	14.791296	-0.062031	4.568688
312.446968	7169.068917	14.796301	-0.062027	4.566212
312.654193	7161.142338	14.801306	-0.062060	4.563770
312.350310	7153.075145	14.806311	-0.061998	4.561283
312.363230	7145.153837	14.811315	-0.061995	4.558839
312.270838	7137.200829	14.816320	-0.061972	4.556384
312.169652	7129.103623	14.821325	-0.061948	4.553883
312.426638	7121.099134	14.826330	-0.061990	4.551410
311.954756	7113.081262	14.831335	-0.061897	4.548931
312.256398	7105.095307	14.836339	-0.061947	4.546461
312.203957	7097.083178	14.841344	-0.061932	4.543981
312.001883	7089.082317	14.846349	-0.061889	4.541503
311.940332	7081.098212	14.851354	-0.061872	4.539030
312.031182	7073.134715	14.856359	-0.061884	4.536561
311.986354	7065.133079	14.861363	-0.061870	4.534079
311.987179	7057.067177	14.866368	-0.061864	4.531576
312.065849	7049.028359	14.871373	-0.061874	4.529080
312.116584	7041.081535	14.876378	-0.061878	4.526611
312.029575	7033.087764	14.881383	-0.061856	4.524126
311.887394	7025.145980	14.886387	-0.061824	4.521655
311.890172	7017.128323	14.891392	-0.061819	4.519160
311.646678	7009.127951	14.896397	-0.061768	4.516668
311.853854	7001.080588	14.901402	-0.061801	4.514162
311.598992	6993.027204	14.906407	-0.061748	4.511651
311.558701	6985.016728	14.911411	-0.061735	4.509152
311.682487	6977.029377	14.916416	-0.061753	4.506660
311.721591	6969.015127	14.921421	-0.061755	4.504158
311.596312	6961.079661	14.926426	-0.061726	4.501678
311.340710	6953.042930	14.931431	-0.061673	4.499165
311.408115	6945.048821	14.936435	-0.061680	4.496665
311.504624	6937.062863	14.941440	-0.061693	4.494166
311.488584	6929.032529	14.946445	-0.061684	4.491652
311.304156	6921.050154	14.951450	-0.061644	4.489151
311.414377	6913.046543	14.956455	-0.061659	4.486642
311.589021	6905.019865	14.961459	-0.061686	4.484125
311.385552	6897.095944	14.966464	-0.061643	4.481638
311.370069	6889.003602	14.971469	-0.061635	4.479097
311.422314	6881.096956	14.976474	-0.061639	4.476613
311.190751	6873.011059	14.981479	-0.061590	4.474070
311.213957	6865.040208	14.986483	-0.061589	4.471563
311.307898	6856.994694	14.991488	-0.061601	4.469032
311.257190	6848.966246	14.996493	-0.061586	4.466504
311.074077	6841.035029	15.001498	-0.061547	4.464004
311.051761	6833.046065	15.006503	-0.061537	4.461486
311.018153	6825.012287	15.011507	-0.061525	4.458951
310.895778	6817.025704	15.016512	-0.061497	4.456430
310.837318	6809.019194	15.021517	-0.061481	4.453902
310.903721	6800.996940	15.026522	-0.061488	4.451367
310.798319	6792.996216	15.031527	-0.061462	4.448838
310.858459	6784.996984	15.036531	-0.061468	4.446308
310.711725	6777.046402	15.041536	-0.061435	4.443791
310.608471	6768.993374	15.046541	-0.061411	4.441240
310.569208	6761.025919	15.051546	-0.061398	4.438715
310.701039	6752.963235	15.056551	-0.061417	4.436160
310.693093	6744.925776	15.061555	-0.061410	4.433610
310.530951	6736.938375	15.066560	-0.061374	4.431074
310.611075	6728.925649	15.071565	-0.061384	4.428529
310.419158	6720.987222	15.076570	-0.061343	4.426006
310.360768	6712.990601	15.081575	-0.061326	4.423463
310.301945	6704.960357	15.086579	-0.061310	4.420908
310.183753	6696.983718	15.091584	-0.061282	4.418368
310.136417	6688.935195	15.096589	-0.061268	4.415804
310.075668	6680.961112	15.101594	-0.061251	4.413263
310.195174	6672.932085	15.106599	-0.061268	4.410703
310.207661	6664.984686	15.111603	-0.061265	4.408167
310.148307	6656.971641	15.116608	-0.061248	4.405609
310.213713	6649.002308	15.121613	-0.061255	4.403063
310.315611	6640.981310	15.126618	-0.061269	4.400500
310.192646	6633.005752	15.131623	-0.061240	4.397949
310.258733	6624.991731	15.136627	-0.061247	4.395385
310.120734	6616.947801	15.141632	-0.061216	4.392809
310.023938	6608.906001	15.146637	-0.061192	4.390232
309.826980	6600.985590	15.151642	-0.061150	4.387692
309.854457	6592.924835	15.156647	-0.061150	4.385106
309.793226	6584.998768	15.161651	-0.061133	4.382562
309.680810	6576.981058	15.166656	-0.061107	4.379987
309.771717	6569.009128	15.171661	-0.061118	4.377426
309.716585	6560.957130	15.176666	-0.061102	4.374837
309.592673	6552.960679	15.181671	-0.061074	4.372264
309.501070	6544.924758	15.186675	-0.061051	4.369676
309.828349	6536.971998	15.191680	-0.061107	4.367117
309.624151	6528.911862	15.196685	-0.061063	4.364518
309.727066	6521.026873	15.201690	-0.061077	4.361976
309.645591	6512.986546	15.206695	-0.061056	4.359382
309.700992	6505.031506	15.211699	-0.061061	4.356814
309.548867	6496.914236	15.216704	-0.061027	4.354191
309.587462	6488.835772	15.221709	-0.061029	4.351580
309.745193	6480.895812	15.226714	-0.061053	4.349013
309.579803	6472.938139	15.231719	-0.061017	4.346437
309.538424	6464.901740	15.236723	-0.061003	4.343834
309.431738	6456.961126	15.241728	-0.060978	4.341261
309.183506	6448.944482	15.246733	-0.060926	4.338660
309.238155	6440.957133	15.251738	-0.060931	4.336069
309.217756	6432.914606	15.256743	-0.060922	4.333459
309.182329	6424.891681	15.261747	-0.060910	4.330853
309.220981	6416.923859	15.266752	-0.060912	4.328264
309.185072	6408.874130	15.271757	-0.060899	4.325646
309.338464	6400.961320	15.276762	-0.060923	4.323072
309.307378	6392.910610	15.281767	-0.060911	4.320451
309.207373	6384.969831	15.286771	-0.060887	4.317864
309.038889	6376.998072	15.291776	-0.060850	4.315264
308.905526	6368.909817	15.296781	-0.060820	4.312625
309.003682	6360.902517	15.301786	-0.060833	4.310012
309.072124	6352.918892	15.306791	-0.060840	4.307406
308.964717	6344.877348	15.311795	-0.060815	4.304778
308.968551	6336.954593	15.316800	-0.060810	4.302187
308.881487	6328.879466	15.321805	-0.060788	4.299545
309.159878	6320.919732	15.326810	-0.060835	4.296941
308.759903	6312.896369	15.331815	-0.060755	4.294310
308.627226	6304.896316	15.336819	-0.060724	4.291687
308.660238	6296.885713	15.341824	-0.060725	4.289060
308.631000	6288.898678	15.346829	-0.060714	4.286439
308.674336	6280.909981	15.351834	-0.060717	4.283816
308.485848	6272.934864	15.356839	-0.060676	4.281194
308.782542	6264.910613	15.361843	-0.060726	4.278559
308.713526	6256.903409	15.366848	-0.060708	4.275924
308.459776	6248.876550	15.371853	-0.060655	4.273280
308.621204	6240.861033	15.376858	-0.060679	4.270641
308.483768	6232.865816	15.381863	-0.060648	4.268005
308.431603	6224.849694	15.386867	-0.060633	4.265361
308.488957	6216.882951	15.391872	-0.060638	4.262732
308.407571	6208.832190	15.396877	-0.060618	4.260073
308.496991	6200.933032	15.401882	-0.060629	4.257464
308.427371	6192.866470	15.406887	-0.060611	4.254797
308.399115	6184.875574	15.411891	-0.060600	4.252153
308.305324	6176.858472	15.416896	-0.060577	4.249498
308.181544	6168.876470	15.421901	-0.060548	4.246853
308.255621	6160.914688	15.426906	-0.060557	4.244215
308.229255	6152.915487	15.431911	-0.060546	4.241562
307.947166	6144.901278	15.436915	-0.060488	4.238900
308.002615	6136.924898	15.441920	-0.060493	4.236252
308.233159	6128.862985	15.446925	-0.060531	4.233576
308.271966	6120.866074	15.451930	-0.060532	4.230917
308.071320	6112.898973	15.456935	-0.060490	4.228265
308.012392	6104.876557	15.461939	-0.060473	4.225594
308.131333	6096.926148	15.466944	-0.060490	4.222946
307.917806	6088.874441	15.471949	-0.060445	4.220261
307.931810	6080.927836	15.476954	-0.060442	4.217610
307.661338	6072.918097	15.481959	-0.060386	4.214934
307.956615	6064.872144	15.486963	-0.060435	4.212250
307.758733	6056.878916	15.491968	-0.060393	4.209577
307.719245	6048.885999	15.496973	-0.060380	4.206904
307.635554	6040.909811	15.501978	-0.060359	4.204235
307.658396	6032.945678	15.506983	-0.060358	4.201568
307.606661	6024.948871	15.511987	-0.060343	4.198889
307.727263	6016.973195	15.516992	-0.060360	4.196216
307.438823	6008.834993	15.521997	-0.060301	4.193483
307.517711	6000.808623	15.527002	-0.060310	4.190790
307.594064	5992.825566	15.532007	-0.060319	4.188110
307.420368	5984.808290	15.537011	-0.060281	4.185413
307.553338	5976.899542	15.542016	-0.060300	4.182755
307.505416	5968.823608	15.547021	-0.060286	4.180036
307.597987	5960.930005	15.552026	-0.060297	4.177379
307.367936	5952.868640	15.557031	-0.060249	4.174660
307.323587	5944.849975	15.562035	-0.060235	4.171956
307.298974	5936.888602	15.567040	-0.060225	4.169269
307.120349	5928.887627	15.572045	-0.060187	4.166566
307.248911	5920.898190	15.577050	-0.060205	4.163868
307.233799	5912.909530	15.582055	-0.060197	4.161168
307.132540	5904.847822	15.587059	-0.060172	4.158439
307.039758	5896.856625	15.592064	-0.060150	4.155733
306.986284	5888.870245	15.597069	-0.060134	4.153027
307.104327	5880.839868	15.602074	-0.060151	4.150307
306.970688	5872.860309	15.607079	-0.060120	4.147599
307.130229	5864.837112	15.612083	-0.060145	4.144878
307.246390	5856.873039	15.617088	-0.060161	4.142174
307.017504	5848.845553	15.622093	-0.060113	4.139443
307.078580	5840.923253	15.627098	-0.060119	4.136750
306.913619	5832.872960	15.632103	-0.060082	4.134009
306.959303	5824.849816	15.637107	-0.060085	4.131277
306.921607	5816.868881	15.642112	-0.060073	4.128557
306.801839	5808.811094	15.647117	-0.060045	4.125808
306.680894	5800.902391	15.652122	-0.060017	4.123108
306.544483	5792.861462	15.657127	-0.059986	4.120361
306.492342	5784.883130	15.662131	-0.059971	4.117635
306.577575	5776.900434	15.667136	-0.059982	4.114907
306.363291	5768.840247	15.672141	-0.059936	4.112147
306.351513	5760.819888	15.677146	-0.059929	4.109401
306.287096	5752.846068	15.682151	-0.059911	4.106669
306.218005	5744.875036	15.687155	-0.059893	4.103935
306.368245	5736.867309	15.692160	-0.059915	4.101190
306.253084	5728.840527	15.697165	-0.059888	4.098434
306.317023	5720.871351	15.702170	-0.059895	4.095697
306.185811	5712.856937	15.707175	-0.059865	4.092941
306.154158	5704.848642	15.712179	-0.059854	4.090186
306.077294	5696.882898	15.717184	-0.059834	4.087443
306.026073	5688.829102	15.722189	-0.059819	4.084669
306.142140	5680.929041	15.727194	-0.059835	4.081948
306.092740	5672.901421	15.732199	-0.059820	4.079178
306.044972	5664.916294	15.737203	-0.059806	4.076422
306.008877	5656.904496	15.742208	-0.059794	4.073655
305.914264	5648.845437	15.747213	-0.059771	4.070868
305.908237	5640.895749	15.752218	-0.059764	4.068119
305.900093	5632.862245	15.757223	-0.059757	4.065339
305.593059	5624.916774	15.762227	-0.059694	4.062583
305.856935	5616.897524	15.767232	-0.059738	4.059808
305.761135	5608.915608	15.772237	-0.059715	4.057039
305.836293	5600.906915	15.777242	-0.059723	4.054261
305.774641	5592.906693	15.782247	-0.059706	4.051482
305.687140	5584.911279	15.787251	-0.059685	4.048702
305.586284	5576.906705	15.792256	-0.059660	4.045918
305.461613	5568.902419	15.797261	-0.059632	4.043131
305.543277	5560.913774	15.802266	-0.059641	4.040350
305.656976	5552.919383	15.807271	-0.059657	4.037566
305.671320	5544.875649	15.812275	-0.059654	4.034762
305.682742	5536.835847	15.817280	-0.059651	4.031957
305.420749	5528.828658	15.822285	-0.059597	4.029157
305.495826	5520.873252	15.827290	-0.059605	4.026378
305.430143	5512.857154	15.832295	-0.059587	4.023574
305.404433	5504.842253	15.837299	-0.059577	4.020770
305.306844	5496.907432	15.842304	-0.059554	4.017990
305.192030	5488.871137	15.847309	-0.059527	4.015172
305.312324	5480.886176	15.852314	-0.059544	4.012374
305.136696	5472.852339	15.857319	-0.059505	4.009552
304.926702	5464.861330	15.862323	-0.059461	4.006743
305.204187	5456.861202	15.867328	-0.059507	4.003937
305.054954	5448.898275	15.872333	-0.059474	4.001134
305.024328	5440.910783	15.877338	-0.059463	3.998323
305.009441	5432.895417	15.882343	-0.059454	3.995501
305.038991	5424.863326	15.887347	-0.059454	3.992671
305.065690	5416.822894	15.892352	-0.059454	3.989836
304.927867	5408.840870	15.897357	-0.059423	3.987017
305.097323	5400.867113	15.902362	-0.059449	3.984204
305.022888	5392.881125	15.907367	-0.059429	3.981381
304.828380	5384.859674	15.912371	-0.059388	3.978541
304.852157	5376.905236	15.917376	-0.059387	3.975727
304.735078	5368.887272	15.922381	-0.059359	3.972885
304.717798	5360.881829	15.927386	-0.059351	3.970048
304.839691	5352.896636	15.932391	-0.059368	3.967218
304.750902	5344.872619	15.937395	-0.059346	3.964369
304.646772	5336.950058	15.942400	-0.059321	3.961554
304.518278	5328.937755	15.947405	-0.059292	3.958704
304.745071	5320.922034	15.952410	-0.059329	3.955857
304.483701	5312.901452	15.957415	-0.059274	3.952998
304.345453	5304.861525	15.962419	-0.059243	3.950132
304.547827	5296.906300	15.967424	-0.059275	3.947300
304.450661	5288.895274	15.972429	-0.059252	3.944441
304.595369	5280.956013	15.977434	-0.059273	3.941610
304.516118	5272.953965	15.982439	-0.059253	3.938750
304.538880	5264.937866	15.987443	-0.059252	3.935885
304.565902	5256.939603	15.992448	-0.059251	3.933024
304.346386	5248.907177	15.997453	-0.059205	3.930145
304.306795	5240.958821	16.002458	-0.059192	3.927296
304.352852	5232.956226	16.007463	-0.059195	3.924428
304.222389	5224.967529	16.012467	-0.059166	3.921560
304.200091	5216.980986	16.017472	-0.059156	3.918692
304.288024	5208.930412	16.022477	-0.059167	3.915801
304.241324	5200.939511	16.027482	-0.059153	3.912927
304.031773	5192.919508	16.032487	-0.059108	3.910037
304.143759	5184.927953	16.037491	-0.059124	3.907161
304.259595	5176.974087	16.042496	-0.059140	3.904297
303.793250	5168.975771	16.047501	-0.059047	3.901404
304.026755	5160.966133	16.052506	-0.059085	3.898518
303.970657	5152.958479	16.057511	-0.059069	3.895625
303.972792	5144.959791	16.062515	-0.059064	3.892734
303.716114	5136.946183	16.067520	-0.059011	3.889830
303.835363	5128.960168	16.072525	-0.059028	3.886942
303.943597	5120.947894	16.077530	-0.059043	3.884041
303.748672	5112.970636	16.082535	-0.059001	3.881146
303.778537	5104.968472	16.087539	-0.059001	3.878243
303.719142	5096.996857	16.092544	-0.058984	3.875348
303.290949	5088.771948	16.097549	-0.058899	3.872351
303.477890	5080.772666	16.102554	-0.058928	3.869446
303.565349	5072.827599	16.107559	-0.058939	3.866557
303.619363	5064.864553	16.112563	-0.058944	3.863658
303.527301	5056.952274	16.117568	-0.058921	3.860773
303.313889	5048.949927	16.122573	-0.058876	3.857850
303.322419	5040.965470	16.127578	-0.058872	3.854936
303.128679	5032.964049	16.132583	-0.058831	3.852009
303.304793	5024.914151	16.137587	-0.058858	3.849070
303.371857	5016.965120	16.142592	-0.058865	3.846163
303.166879	5008.970768	16.147597	-0.058821	3.843232
303.164154	5000.990875	16.152602	-0.058815	3.840309
303.304797	4993.008158	16.157607	-0.058836	3.837385
303.179142	4984.955487	16.162611	-0.058807	3.834427
303.157717	4976.989026	16.167616	-0.058798	3.831501
303.073950	4968.952384	16.172621	-0.058777	3.828546
302.945719	4960.969495	16.177626	-0.058747	3.825607
302.957514	4953.010234	16.182631	-0.058744	3.822678
303.034356	4944.992345	16.187635	-0.058753	3.819726
303.119993	4937.058853	16.192640	-0.058763	3.816803
302.968988	4929.025799	16.197645	-0.058730	3.813836
303.056533	4920.996235	16.202650	-0.058741	3.810874
303.078047	4913.022332	16.207655	-0.058739	3.807928
303.048692	4905.001020	16.212659	-0.058728	3.804961
302.749127	4897.114797	16.217664	-0.058667	3.802036
302.856488	4889.044889	16.222669	-0.058681	3.799049
302.712669	4881.084490	16.227674	-0.058649	3.796096
302.515184	4873.045191	16.232679	-0.058607	3.793109
302.526366	4865.006668	16.237683	-0.058604	3.790125
302.724936	4857.030529	16.242688	-0.058635	3.787166
302.616325	4849.026001	16.247693	-0.058609	3.784187
302.592300	4841.046248	16.252698	-0.058599	3.781217
302.501342	4833.043283	16.257703	-0.058577	3.778235
302.307342	4825.033634	16.262707	-0.058535	3.775245
302.228072	4817.059462	16.267712	-0.058515	3.772269
302.169813	4809.032666	16.272717	-0.058499	3.769271
302.373230	4801.041475	16.277722	-0.058531	3.766290
302.165340	4793.070784	16.282727	-0.058487	3.763305
302.153454	4785.066156	16.287731	-0.058479	3.760310
302.257620	4777.108291	16.292736	-0.058493	3.757332
302.223131	4769.042004	16.297741	-0.058481	3.754308
302.301700	4761.031826	16.302746	-0.058491	3.751305
302.303150	4753.049443	16.307751	-0.058485	3.748309
302.191820	4745.013180	16.312755	-0.058459	3.745287
302.117050	4737.100696	16.317760	-0.058440	3.742310
302.074612	4729.082223	16.322765	-0.058427	3.739292
302.077386	4721.080671	16.327770	-0.058422	3.736279
301.812472	4713.114855	16.332775	-0.058367	3.733270
301.875733	4705.054605	16.337779	-0.058373	3.730231
301.968099	4697.092470	16.342784	-0.058385	3.727227
301.821787	4689.080853	16.347789	-0.058352	3.724197
301.820521	4681.163144	16.352794	-0.058346	3.721203
302.046630	4673.133372	16.357799	-0.058383	3.718169
301.875603	4665.139648	16.362803	-0.058346	3.715138
301.699979	4657.067207	16.367808	-0.058307	3.712073
301.493289	4649.038070	16.372813	-0.058264	3.709022
301.619299	4641.059038	16.377818	-0.058282	3.705996
301.679346	4633.094042	16.382823	-0.058287	3.702971
301.165260	4625.120396	16.387827	-0.058186	3.699925
301.360239	4617.167101	16.392832	-0.058217	3.696903
301.247107	4609.151933	16.397837	-0.058190	3.693847
301.191238	4601.146243	16.402842	-0.058175	3.690793
301.113636	4593.159273	16.407847	-0.058155	3.687744
301.037268	4585.149450	16.412851	-0.058135	3.684683
301.101963	4577.218628	16.417856	-0.058142	3.681653
301.008738	4569.197116	16.422861	-0.058119	3.678582
301.187562	4561.181337	16.427866	-0.058146	3.675518
300.801519	4553.159431	16.432871	-0.058069	3.672435
300.872930	4545.151207	16.437875	-0.058077	3.669365
301.116599	4537.194183	16.442880	-0.058117	3.666318
300.859322	4529.201893	16.447885	-0.058064	3.663241
300.875264	4521.195530	16.452890	-0.058061	3.660163
300.795307	4513.208080	16.457895	-0.058041	3.657088
300.850181	4505.163929	16.462899	-0.058045	3.653991
300.656232	4497.214799	16.467904	-0.058004	3.650922
300.564219	4489.191047	16.472909	-0.057981	3.647825
300.598222	4481.174407	16.477914	-0.057982	3.644731
300.648007	4473.266855	16.482919	-0.057986	3.641676
300.500201	4465.218163	16.487923	-0.057953	3.638560
300.736523	4457.234527	16.492928	-0.057991	3.635476
300.607327	4449.205585	16.497933	-0.057962	3.632362
300.615132	4441.181307	16.502938	-0.057958	3.629251
300.652355	4433.180357	16.507943	-0.057959	3.626147
300.471092	4425.236881	16.512947	-0.057920	3.623057
300.561360	4417.222623	16.517952	-0.057931	3.619944
300.492159	4409.260929	16.522957	-0.057913	3.616844
300.612062	4401.223041	16.527962	-0.057930	3.613717
300.637392	4393.229176	16.532967	-0.057929	3.610603
300.530955	4385.239547	16.537971	-0.057904	3.607483
300.567109	4377.259534	16.542976	-0.057905	3.604369
300.353761	4369.328953	16.547981	-0.057860	3.601264
300.228118	4361.332815	16.552986	-0.057831	3.598133
300.286237	4353.312192	16.557991	-0.057836	3.594995
300.192676	4345.281573	16.562995	-0.057814	3.591846
300.236378	4337.315801	16.568000	-0.057816	3.588724
300.027035	4329.303668	16.573005	-0.057772	3.585574
300.078178	4321.344951	16.578010	-0.057776	3.582449
300.054547	4313.350173	16.583015	-0.057766	3.579305
299.831598	4305.392816	16.588019	-0.057719	3.576167
300.000216	4297.366411	16.593024	-0.057745	3.573011
300.044546	4289.326047	16.598029	-0.057748	3.569843
299.933857	4281.361136	16.603034	-0.057722	3.566697
299.728621	4273.373127	16.608039	-0.057678	3.563537
299.763295	4265.359595	16.613043	-0.057679	3.560370
299.867618	4257.386682	16.618048	-0.057693	3.557219
299.780083	4249.341238	16.623053	-0.057671	3.554031
299.808726	4241.276307	16.628058	-0.057671	3.550836
299.778800	4233.328417	16.633063	-0.057660	3.547682
299.533700	4225.322743	16.638067	-0.057609	3.544496
299.769845	4217.374691	16.643072	-0.057647	3.541345
299.751197	4209.348409	16.648077	-0.057638	3.538152
299.657397	4201.356215	16.653082	-0.057615	3.534968
299.633670	4193.388691	16.658087	-0.057606	3.531792
299.622712	4185.373391	16.663091	-0.057598	3.528595
299.612075	4177.393485	16.668096	-0.057591	3.525410
299.228474	4169.437479	16.673101	-0.057514	3.522219
299.450928	4161.434025	16.678106	-0.057550	3.519026
299.455729	4153.452056	16.683111	-0.057545	3.515831
299.427290	4145.416023	16.688115	-0.057534	3.512610
299.431471	4137.416777	16.693120	-0.057530	3.509403
299.485291	4129.419467	16.698125	-0.057534	3.506195
299.375114	4121.473204	16.703130	-0.057508	3.502999
299.386062	4113.456569	16.708135	-0.057505	3.499776
299.179613	4105.500647	16.713139	-0.057461	3.496567
299.223437	4097.500106	16.718144	-0.057464	3.493346
298.992496	4089.483490	16.723149	-0.057415	3.490106
298.927599	4081.497005	16.728154	-0.057398	3.486881
299.041627	4073.513179	16.733159	-0.057413	3.483659
298.846577	4065.541702	16.738163	-0.057372	3.480430
299.041240	4057.573986	16.743168	-0.057402	3.477211
298.938265	4049.546183	16.748173	-0.057378	3.473956
298.928187	4041.503977	16.753178	-0.057370	3.470695
298.644593	4033.545652	16.758183	-0.057312	3.467456
298.557287	4025.539329	16.763187	-0.057290	3.464200
299.007710	4017.538343	16.768192	-0.057369	3.460962
298.829439	4009.563498	16.773197	-0.057330	3.457710
298.666996	4001.557440	16.778202	-0.057294	3.454443
298.692418	3993.574547	16.783207	-0.057294	3.451189
298.711449	3985.561466	16.788211	-0.057292	3.447919
298.467364	3977.580288	16.793216	-0.057241	3.444650
298.579114	3969.633704	16.798221	-0.057256	3.441404
298.604172	3961.627656	16.803226	-0.057255	3.438128
298.364175	3953.630991	16.808231	-0.057205	3.434844
298.440397	3945.580545	16.813235	-0.057214	3.431545
298.521188	3937.594451	16.818240	-0.057223	3.428269
298.350795	3929.591728	16.823245	-0.057186	3.424975
298.358082	3921.640620	16.828250	-0.057182	3.421705
298.281677	3913.656250	16.833255	-0.057163	3.418415
298.212350	3905.663120	16.838259	-0.057144	3.415119
298.173764	3897.666881	16.843264	-0.057131	3.411819
298.000926	3889.659298	16.848269	-0.057094	3.408507
298.240519	3881.654011	16.853274	-0.057133	3.405207
298.191042	3873.708360	16.858279	-0.057118	3.401918
298.047595	3865.731543	16.863283	-0.057086	3.398610
298.276193	3857.731438	16.868288	-0.057123	3.395302
297.932527	3849.653141	16.873293	-0.057054	3.391939
297.765376	3841.667368	16.878298	-0.057017	3.388616
297.881558	3833.659636	16.883303	-0.057033	3.385291
297.733940	3825.706743	16.888307	-0.057000	3.381977
297.620808	3817.751311	16.893312	-0.056974	3.378659
297.416460	3809.749372	16.898317	-0.056930	3.375315
297.508810	3801.761641	16.903322	-0.056942	3.371985
297.660272	3793.741620	16.908327	-0.056965	3.368639
297.449282	3785.758217	16.913331	-0.056920	3.365293
297.704607	3777.801833	16.918336	-0.056962	3.361972
297.466084	3769.803221	16.923341	-0.056912	3.358611
297.407847	3761.800206	16.928346	-0.056896	3.355252
297.482432	3753.798251	16.933351	-0.056904	3.351895
297.394334	3745.793833	16.938355	-0.056882	3.348528
297.517290	3737.804461	16.943360	-0.056900	3.345171
297.465016	3729.841963	16.948365	-0.056885	3.341816
297.695577	3721.827369	16.953370	-0.056922	3.338446
297.393601	3713.873826	16.958375	-0.056861	3.335078
297.177397	3705.868524	16.963379	-0.056815	3.331689
297.246187	3697.867932	16.968384	-0.056822	3.328308
297.143043	3689.880939	16.973389	-0.056797	3.324924
296.862052	3681.927343	16.978394	-0.056740	3.321543
296.997810	3673.925399	16.983399	-0.056759	3.318154
297.116136	3665.903711	16.988403	-0.056776	3.314753
296.906185	3657.908244	16.993408	-0.056731	3.311347
296.890197	3649.900239	16.998413	-0.056723	3.307939
296.976445	3641.874560	17.003418	-0.056734	3.304524
297.012206	3633.931903	17.008423	-0.056735	3.301139
296.820533	3625.976005	17.013427	-0.056694	3.297737
296.832640	3617.980238	17.018432	-0.056690	3.294321
296.709916	3609.973475	17.023437	-0.056662	3.290892
296.735049	3601.990992	17.028442	-0.056661	3.287476
296.756133	3593.997505	17.033447	-0.056660	3.284051
296.618455	3586.026676	17.038451	-0.056629	3.280626
296.535335	3578.074567	17.043456	-0.056608	3.277208
296.609213	3570.035278	17.048461	-0.056616	3.273755
296.620084	3562.018138	17.053466	-0.056613	3.270305
296.601142	3554.053456	17.058471	-0.056604	3.266873
296.359738	3546.054498	17.063475	-0.056553	3.263414
296.624088	3538.072127	17.068480	-0.056597	3.259978
296.549838	3530.108122	17.073485	-0.056578	3.256533
296.494763	3522.092403	17.078490	-0.056562	3.253063
296.312953	3514.073149	17.083495	-0.056523	3.249583
296.384554	3506.100397	17.088499	-0.056531	3.246129
296.330212	3498.144857	17.093504	-0.056515	3.242674
296.331419	3490.134514	17.098509	-0.056510	3.239193
296.303365	3482.175672	17.103514	-0.056499	3.235730
296.075385	3474.136457	17.108519	-0.056451	3.232221
295.970106	3466.115421	17.113523	-0.056426	3.228720
296.057676	3458.123755	17.118528	-0.056437	3.225236
295.897893	3450.180961	17.123533	-0.056402	3.221760
295.928540	3442.172609	17.128538	-0.056402	3.218259
295.882853	3434.229307	17.133543	-0.056388	3.214779
296.122494	3426.173092	17.138547	-0.056427	3.211258
295.780375	3418.236639	17.143552	-0.056358	3.207762
295.574858	3410.246375	17.148557	-0.056314	3.204244
295.774610	3402.262101	17.153562	-0.056346	3.200741
295.809434	3394.295032	17.158567	-0.056347	3.197235
295.550234	3386.291003	17.163571	-0.056293	3.193697
295.664313	3378.285170	17.168576	-0.056309	3.190170
295.638460	3370.273945	17.173581	-0.056299	3.186631
295.477663	3362.306420	17.178586	-0.056263	3.183101
295.456827	3354.336517	17.183591	-0.056254	3.179572
295.489454	3346.338656	17.188595	-0.056255	3.176029
295.417039	3338.352078	17.193600	-0.056236	3.172483
295.227597	3330.372405	17.198605	-0.056195	3.168931
295.349316	3322.347154	17.203610	-0.056212	3.165368
295.663972	3314.385807	17.208615	-0.056265	3.161837
295.308988	3306.419733	17.213619	-0.056194	3.158272
295.426553	3298.421103	17.218624	-0.056210	3.154708
295.428921	3290.400759	17.223629	-0.056205	3.151126
295.008921	3282.417493	17.228634	-0.056121	3.147538
294.994854	3274.459615	17.233639	-0.056113	3.143975
295.079119	3266.431515	17.238643	-0.056124	3.140381
295.182521	3258.482317	17.243648	-0.056137	3.136818
295.015463	3250.492292	17.248653	-0.056101	3.133222
294.837689	3242.487607	17.253658	-0.056062	3.129614
295.107238	3234.524310	17.258663	-0.056107	3.126041
294.848282	3226.555126	17.263667	-0.056053	3.122437
294.838120	3218.581678	17.268672	-0.056046	3.118838
294.940198	3210.584194	17.273677	-0.056059	3.115229
294.819090	3202.549846	17.278682	-0.056031	3.111590
294.771269	3194.587246	17.283687	-0.056017	3.107982
294.819775	3186.558918	17.288691	-0.056021	3.104344
294.783232	3178.622731	17.293696	-0.056008	3.100740
294.629351	3170.655378	17.298701	-0.055974	3.097112
294.606264	3162.639723	17.303706	-0.055964	3.093464
294.914136	3154.625566	17.308711	-0.056016	3.089828
294.535639	3146.663236	17.313715	-0.055940	3.086179
294.590711	3138.682420	17.318720	-0.055945	3.082537
294.389168	3130.724706	17.323725	-0.055902	3.078890
294.329177	3122.736262	17.328730	-0.055886	3.075231
294.121738	3114.674293	17.333735	-0.055841	3.071527
294.195608	3106.651999	17.338739	-0.055850	3.067850
294.232992	3098.709581	17.343744	-0.055851	3.064204
294.215660	3090.719097	17.348749	-0.055843	3.060528
293.977138	3082.772395	17.353754	-0.055793	3.056858
294.099511	3074.777351	17.358759	-0.055810	3.053178
293.930236	3066.777250	17.363763	-0.055773	3.049478
293.984349	3058.823359	17.368768	-0.055778	3.045805
293.922888	3050.828246	17.373773	-0.055761	3.042102
294.188187	3042.851557	17.378778	-0.055805	3.038420
294.016829	3034.892626	17.383783	-0.055767	3.034721
293.991094	3026.862533	17.388787	-0.055757	3.030990
294.185945	3018.871086	17.393792	-0.055788	3.027284
294.001407	3010.912752	17.398797	-0.055748	3.023571
293.897000	3002.927146	17.403802	-0.055723	3.019844
293.834021	2994.976544	17.408807	-0.055706	3.016130
293.654639	2986.959811	17.413811	-0.055667	3.012376
293.885259	2978.973512	17.418816	-0.055705	3.008651
293.772299	2970.983807	17.423821	-0.055678	3.004903
293.619600	2963.045572	17.428826	-0.055644	3.001172
293.637894	2955.078651	17.433831	-0.055642	2.997432
293.614258	2947.032528	17.438835	-0.055632	2.993648
293.812629	2939.023459	17.443840	-0.055664	2.989888
293.546373	2931.059086	17.448845	-0.055609	2.986120
293.473071	2923.086384	17.453850	-0.055590	2.982354
293.446039	2915.120188	17.458855	-0.055579	2.978588
293.470209	2907.105868	17.463859	-0.055578	2.974797
293.209308	2899.146042	17.468864	-0.055524	2.971013
293.269303	2891.150965	17.473869	-0.055530	2.967224
293.328948	2883.173336	17.478874	-0.055535	2.963438
293.228682	2875.217146	17.483879	-0.055511	2.959649
293.131524	2867.256450	17.488883	-0.055488	2.955853
293.145301	2859.254810	17.493888	-0.055485	2.952039
293.115803	2851.229622	17.498893	-0.055474	2.948206
292.856202	2843.265239	17.503898	-0.055420	2.944385
293.057880	2835.299140	17.508903	-0.055452	2.940582
292.899128	2827.323789	17.513907	-0.055417	2.936752
292.961179	2819.325160	17.518912	-0.055423	2.932916
292.992539	2811.314985	17.523917	-0.055424	2.929069
293.019392	2803.335265	17.528922	-0.055423	2.925231
292.902249	2795.403122	17.533927	-0.055396	2.921403
292.645621	2787.427520	17.538931	-0.055343	2.917541
292.624624	2779.436110	17.543936	-0.055333	2.913680
292.740156	2771.337100	17.548941	-0.055349	2.909768
292.674207	2763.366812	17.553946	-0.055332	2.905904
292.676386	2755.445319	17.558951	-0.055327	2.902062
292.479317	2747.459331	17.563955	-0.055284	2.898173
292.290983	2739.515279	17.568960	-0.055244	2.894300
292.426376	2731.490322	17.573965	-0.055264	2.890399
292.381321	2723.516008	17.578970	-0.055250	2.886508
292.294589	2715.562860	17.583975	-0.055228	2.882620
291.977431	2707.620654	17.588979	-0.055164	2.878719
292.291832	2699.604838	17.593984	-0.055217	2.874812
292.099796	2691.610588	17.598989	-0.055176	2.870882
292.092767	2683.610469	17.603994	-0.055169	2.866954
292.218568	2675.646390	17.608999	-0.055187	2.863045
292.114021	2667.663251	17.614003	-0.055162	2.859109
292.083718	2659.718240	17.619008	-0.055151	2.855191
292.191332	2651.703497	17.624013	-0.055165	2.851240
292.222493	2643.705289	17.629018	-0.055166	2.847288
292.203903	2635.767290	17.634023	-0.055157	2.843358
291.793512	2627.815480	17.639027	-0.055075	2.839393
291.928234	2619.840101	17.644032	-0.055095	2.835441
291.984679	2611.811245	17.649037	-0.055100	2.831453
291.798869	2603.826924	17.654042	-0.055059	2.827468
291.820631	2595.857173	17.659047	-0.055058	2.823496
291.662440	2587.886083	17.664051	-0.055023	2.819508
291.682186	2579.930937	17.669056	-0.055021	2.815532
291.639392	2571.916920	17.674061	-0.055008	2.811517
291.602165	2563.936757	17.679066	-0.054996	2.807514
291.613688	2555.980404	17.684071	-0.054992	2.803520
291.693100	2547.984118	17.689075	-0.055002	2.799504
291.762365	2540.042568	17.694080	-0.055009	2.795510
291.711712	2532.035873	17.699085	-0.054994	2.791470
291.607118	2524.051376	17.704090	-0.054969	2.787432
291.625690	2516.087032	17.709095	-0.054967	2.783405
291.641253	2508.106830	17.714099	-0.054965	2.779365
291.441178	2500.171341	17.719104	-0.054922	2.775328
291.393696	2492.171964	17.724109	-0.054908	2.771262
291.227959	2484.201240	17.729114	-0.054871	2.767198
291.347957	2476.226015	17.734119	-0.054888	2.763143
290.933914	2468.284694	17.739123	-0.054806	2.759067
291.024766	2460.305806	17.744128	-0.054817	2.754996
291.227915	2452.204115	17.749133	-0.054849	2.750862
291.145458	2444.234592	17.754138	-0.054829	2.746774
291.125224	2436.287265	17.759143	-0.054819	2.742694
290.867147	2428.328908	17.764147	-0.054766	2.738588
290.863171	2420.384661	17.769152	-0.054760	2.734498
290.842379	2412.356863	17.774157	-0.054750	2.730358
290.914870	2404.384550	17.779162	-0.054758	2.726247
290.944276	2396.453483	17.784167	-0.054758	2.722147
290.678731	2388.503235	17.789171	-0.054704	2.718014
290.738841	2380.527554	17.794176	-0.054709	2.713881
290.743509	2372.508758	17.799181	-0.054705	2.709716
290.800653	2364.527184	17.804186	-0.054710	2.705567
290.536464	2356.601157	17.809191	-0.054655	2.701421
290.570310	2348.606801	17.814195	-0.054656	2.697251
290.611193	2340.645428	17.819200	-0.054658	2.693093
290.399308	2332.655877	17.824205	-0.054613	2.688897
290.494188	2324.663895	17.829210	-0.054626	2.684713
290.431306	2316.745574	17.834215	-0.054608	2.680551
290.329422	2308.765418	17.839219	-0.054584	2.676347
290.329208	2300.764201	17.844224	-0.054579	2.672133
290.409438	2292.751049	17.849229	-0.054588	2.667910
290.296505	2284.798838	17.854234	-0.054562	2.663701
290.089145	2276.863698	17.859239	-0.054517	2.659488
290.189816	2268.878927	17.864243	-0.054531	2.655261
290.211752	2260.859444	17.869248	-0.054529	2.651005
290.046854	2252.918529	17.874253	-0.054493	2.646771
290.040421	2244.942571	17.879258	-0.054487	2.642522
289.960876	2237.009475	17.884263	-0.054466	2.638285
290.024798	2229.030067	17.889267	-0.054473	2.634025
289.897586	2221.033172	17.894272	-0.054444	2.629736
290.130559	2213.040720	17.899277	-0.054482	2.625467
289.895164	2205.106543	17.904282	-0.054432	2.621190
289.881883	2197.148376	17.909287	-0.054424	2.616909
289.792807	2189.153868	17.914291	-0.054402	2.612596
289.835705	2181.178185	17.919296	-0.054405	2.608295
289.626150	2173.234049	17.924301	-0.054360	2.603987
289.383546	2165.293759	17.929306	-0.054310	2.599671
289.628652	2157.315427	17.934311	-0.054350	2.595361
289.489447	2149.152178	17.939315	-0.054318	2.590916
289.481507	2141.202693	17.944320	-0.054312	2.586590
289.543831	2133.260562	17.949325	-0.054318	2.582265
289.407627	2125.325200	17.954330	-0.054287	2.577923
289.355683	2117.395541	17.959335	-0.054272	2.573582
289.353280	2109.391056	17.964339	-0.054266	2.569197
289.474618	2101.429533	17.969344	-0.054283	2.564836
289.201230	2093.519421	17.974349	-0.054227	2.560469
289.199094	2085.558340	17.979354	-0.054221	2.556085
289.233003	2077.576094	17.984359	-0.054222	2.551684
289.106886	2069.595723	17.989363	-0.054193	2.547265
289.010520	2061.640424	17.994368	-0.054169	2.542855
288.965607	2053.678086	17.999373	-0.054156	2.538437
289.105208	2045.701058	18.004378	-0.054176	2.534016
288.883357	2037.752055	18.009383	-0.054129	2.529577
288.806878	2029.788754	18.014387	-0.054110	2.525133
288.872646	2021.828282	18.019392	-0.054116	2.520692
288.699403	2013.898782	18.024397	-0.054079	2.516244
288.561221	2005.884831	18.029402	-0.054048	2.511743
288.828011	1997.871290	18.034407	-0.054092	2.507264
288.654883	1989.924138	18.039411	-0.054054	2.502782
288.508814	1981.992815	18.044416	-0.054021	2.498303
288.556384	1974.022042	18.049421	-0.054025	2.493807
288.317074	1966.053633	18.054426	-0.053975	2.489284
288.411336	1958.088557	18.059431	-0.053987	2.484779
288.252291	1950.159471	18.064435	-0.053952	2.480268
288.284555	1942.190686	18.069440	-0.053953	2.475739
288.212239	1934.205709	18.074445	-0.053934	2.471186
288.124094	1926.229626	18.079450	-0.053912	2.466628
288.317968	1918.262887	18.084455	-0.053942	2.462088
288.135270	1910.317746	18.089459	-0.053903	2.457524
287.994232	1902.378485	18.094464	-0.053871	2.452958
288.049267	1894.393382	18.099469	-0.053876	2.448371
288.015006	1886.418951	18.104474	-0.053864	2.443776
288.002271	1878.492109	18.109479	-0.053856	2.439200
287.936818	1870.529895	18.114483	-0.053839	2.434592
287.875333	1862.481841	18.119488	-0.053822	2.429926
287.756042	1854.542101	18.124493	-0.053794	2.425309
287.758519	1846.588028	18.129498	-0.053789	2.420684
288.022882	1838.616860	18.134503	-0.053833	2.416061
287.791135	1830.673427	18.139507	-0.053784	2.411406
287.584269	1822.739233	18.144512	-0.053740	2.406750
287.622457	1814.776997	18.149517	-0.053742	2.402088
287.539860	1806.832737	18.154522	-0.053721	2.397417
287.734733	1798.842320	18.159527	-0.053752	2.392732
287.594246	1790.880749	18.164531	-0.053720	2.388028
287.605383	1782.922314	18.169536	-0.053717	2.383329
287.750353	1774.968210	18.174541	-0.053739	2.378634
287.468609	1767.042529	18.179546	-0.053681	2.373913
287.419758	1759.067626	18.184551	-0.053666	2.369171
287.309955	1751.119274	18.189555	-0.053640	2.364431
287.345901	1743.183749	18.194560	-0.053642	2.359700
287.245483	1735.248592	18.199565	-0.053617	2.354949
287.276517	1727.219296	18.204570	-0.053618	2.350143
287.257904	1719.272882	18.209575	-0.053609	2.345373
287.143597	1711.323714	18.214579	-0.053582	2.340583
287.313337	1703.358532	18.219584	-0.053608	2.335798
287.225689	1695.412519	18.224589	-0.053587	2.330993
287.008364	1687.472757	18.229594	-0.053541	2.326171
287.086334	1679.529397	18.234599	-0.053550	2.321361
286.931400	1671.593425	18.239603	-0.053515	2.316526
286.773672	1663.624808	18.244608	-0.053481	2.311662
286.695406	1655.678283	18.249613	-0.053461	2.306806
286.640432	1647.708610	18.254618	-0.053445	2.301929
286.873296	1639.754767	18.259623	-0.053483	2.297075
286.827943	1631.783185	18.264627	-0.053469	2.292176
286.829770	1623.835346	18.269632	-0.053464	2.287286
286.891733	1615.884063	18.274637	-0.053470	2.282388
286.523617	1607.994789	18.279642	-0.053396	2.277481
286.584534	1599.990676	18.284647	-0.053402	2.272529
286.519384	1591.986740	18.289651	-0.053384	2.267556
286.355401	1584.061477	18.294656	-0.053348	2.262612
286.538691	1576.109676	18.299661	-0.053377	2.257670
286.447827	1568.161846	18.304666	-0.053355	2.252697
286.398595	1560.228312	18.309671	-0.053340	2.247725
286.168813	1552.292301	18.314675	-0.053292	2.242725
286.094028	1544.368861	18.319680	-0.053272	2.237735
286.336394	1536.372542	18.324685	-0.053312	2.232715
286.254195	1528.411812	18.329690	-0.053291	2.227679
286.104718	1520.503678	18.334695	-0.053258	2.222658
286.072146	1512.555819	18.339699	-0.053247	2.217611
286.131859	1504.596176	18.344704	-0.053252	2.212553
286.041486	1496.657949	18.349709	-0.053230	2.207484
285.942933	1488.706463	18.354714	-0.053206	2.202394
286.124475	1480.782327	18.359719	-0.053235	2.197335
285.987340	1472.828557	18.364723	-0.053204	2.192216
285.964221	1464.859622	18.369728	-0.053194	2.187086
285.835090	1456.939154	18.374733	-0.053164	2.181965
285.548225	1449.024770	18.379738	-0.053106	2.176822
285.649541	1441.057763	18.384743	-0.053119	2.171668
285.713920	1433.097553	18.389747	-0.053126	2.166503
285.564268	1425.186758	18.394752	-0.053092	2.161338
285.516059	1417.267831	18.399757	-0.053078	2.156165
285.438109	1409.305693	18.404762	-0.053058	2.150948
285.563197	1401.343374	18.409767	-0.053076	2.145737
285.471557	1393.407856	18.414771	-0.053053	2.140511
285.334294	1385.498075	18.419776	-0.053022	2.135285
285.544886	1377.522856	18.424781	-0.053056	2.130036
285.320502	1369.601435	18.429786	-0.053009	2.124768
285.288214	1361.692102	18.434791	-0.052997	2.119513
285.189250	1353.753214	18.439795	-0.052974	2.114219
285.311121	1345.721774	18.444800	-0.052991	2.108871
285.193587	1337.811627	18.449805	-0.052963	2.103568
285.046119	1329.898402	18.454810	-0.052931	2.098246
285.013164	1321.977612	18.459815	-0.052919	2.092917
284.914253	1314.023442	18.464819	-0.052895	2.087545
284.752979	1306.124930	18.469824	-0.052860	2.082191
284.692938	1298.218298	18.474829	-0.052843	2.076827
284.619191	1290.252879	18.479834	-0.052824	2.071408
284.605382	1282.311264	18.484839	-0.052816	2.065997
284.709439	1274.369340	18.489843	-0.052830	2.060584
284.758016	1266.440366	18.494848	-0.052834	2.055159
284.561583	1258.512077	18.499853	-0.052792	2.049696
284.689465	1250.567441	18.504858	-0.052810	2.044240
284.683144	1242.671739	18.509863	-0.052803	2.038789
284.577545	1234.749791	18.514867	-0.052778	2.033296
284.142362	1226.845286	18.519872	-0.052692	2.027766
284.281899	1218.886647	18.524877	-0.052712	2.022242
284.214136	1210.963026	18.529882	-0.052694	2.016706
284.220015	1203.024906	18.534887	-0.052690	2.011152
284.099740	1195.104474	18.539891	-0.052662	2.005583
284.230563	1187.179973	18.544896	-0.052681	2.000021
283.941540	1179.313409	18.549901	-0.052622	1.994440
283.829161	1171.352487	18.554906	-0.052596	1.988795
283.871400	1163.430105	18.559911	-0.052598	1.983178
283.684415	1155.534689	18.564915	-0.052558	1.977540
283.658556	1147.600085	18.569920	-0.052548	1.971875
283.614030	1139.669283	18.574925	-0.052534	1.966195
283.866347	1131.726350	18.579930	-0.052575	1.960521
283.749059	1123.843123	18.584935	-0.052548	1.954834
283.811652	1115.846679	18.589939	-0.052554	1.949067
283.635545	1107.957233	18.594944	-0.052516	1.943336
283.529611	1100.063672	18.599949	-0.052491	1.937592
283.487666	1092.128947	18.604954	-0.052478	1.931808
283.580014	1084.201590	18.609959	-0.052489	1.926026
283.368463	1076.326348	18.614963	-0.052445	1.920232
283.196390	1068.436821	18.619968	-0.052407	1.914414
283.163488	1060.493463	18.624973	-0.052396	1.908554
283.178561	1052.570811	18.629978	-0.052393	1.902697
283.345409	1044.645917	18.634983	-0.052419	1.896837
283.116107	1036.752295	18.639987	-0.052371	1.890938
283.077819	1028.843149	18.644992	-0.052358	1.885030
282.958919	1020.978980	18.649997	-0.052331	1.879128
283.035163	1013.041986	18.655002	-0.052339	1.873175
282.974235	1005.119206	18.660007	-0.052323	1.867198
282.835880	997.229521	18.665011	-0.052291	1.861218
282.690436	989.344169	18.670016	-0.052259	1.855221
282.713219	981.419301	18.675021	-0.052258	1.849194
282.835375	973.486186	18.680026	-0.052275	1.843152
282.670776	965.631931	18.685031	-0.052239	1.837118
282.566727	957.716394	18.690035	-0.052214	1.831023
282.554142	949.806511	18.695040	-0.052207	1.824924
282.445339	941.931834	18.700045	-0.052181	1.818819
282.380489	934.029280	18.705050	-0.052163	1.812678
282.511033	926.109920	18.710055	-0.052182	1.806526
282.529582	918.219549	18.715059	-0.052180	1.800363
282.331582	910.364647	18.720064	-0.052138	1.794179
282.426730	902.393456	18.725069	-0.052150	1.787919
282.117047	894.531278	18.730074	-0.052087	1.781673
282.061650	886.667402	18.735079	-0.052072	1.775435
282.143702	878.747650	18.740083	-0.052081	1.769147
282.287711	870.835924	18.745088	-0.052103	1.762851
282.073890	863.002873	18.750093	-0.052058	1.756551
281.770999	855.123787	18.755098	-0.051996	1.750180
282.006160	847.209734	18.760103	-0.052034	1.743826
281.989298	839.331787	18.765107	-0.052026	1.737445
281.912020	831.454639	18.770112	-0.052006	1.731034
281.867353	823.579227	18.775117	-0.051992	1.724604
281.778486	815.719571	18.780122	-0.051970	1.718158
281.668355	807.842360	18.785127	-0.051944	1.711670
281.600289	799.945567	18.790131	-0.051926	1.705147
281.370262	792.109451	18.795136	-0.051878	1.698628
281.375364	784.228775	18.800141	-0.051874	1.692077
281.116663	776.366325	18.805146	-0.051820	1.685481
281.309860	768.480588	18.810151	-0.051851	1.678900
281.410335	760.581690	18.815155	-0.051864	1.672270
281.135903	752.737678	18.820160	-0.051808	1.665609
281.054203	744.896470	18.825165	-0.051787	1.658950
281.179009	736.992239	18.830170	-0.051805	1.652238
281.236120	729.124705	18.835175	-0.051810	1.645521
281.088806	721.294732	18.840179	-0.051777	1.638781
280.994050	713.418714	18.845184	-0.051754	1.631980
280.924107	705.534151	18.850189	-0.051736	1.625147
280.834123	697.686860	18.855194	-0.051714	1.618314
280.989844	689.812121	18.860199	-0.051737	1.611464
280.756526	681.988091	18.865203	-0.051688	1.604573
280.890023	674.123353	18.870208	-0.051708	1.597669
280.893529	666.271722	18.875213	-0.051703	1.590728
280.676113	658.440387	18.880218	-0.051657	1.583743
280.621708	650.622552	18.885223	-0.051642	1.576762
280.398929	642.796428	18.890227	-0.051595	1.569719
280.331726	634.960039	18.895232	-0.051577	1.562657
280.516354	627.104892	18.900237	-0.051606	1.555583
280.269395	619.263508	18.905242	-0.051555	1.548426
280.238525	611.435658	18.910247	-0.051544	1.541280
280.219664	603.604734	18.915251	-0.051535	1.534099
280.194007	595.754695	18.920256	-0.051525	1.526866
280.036039	587.967028	18.925261	-0.051490	1.519636
280.039389	580.130103	18.930266	-0.051485	1.512351
280.065714	572.293763	18.935271	-0.051485	1.505034
279.897562	564.504107	18.940275	-0.051448	1.497695
279.807681	556.679694	18.945280	-0.051426	1.490300
279.821732	548.869403	18.950285	-0.051423	1.482897
279.767371	541.061492	18.955290	-0.051408	1.475448
279.701141	533.208917	18.960295	-0.051390	1.467917
279.570873	525.418782	18.965299	-0.051361	1.460397
279.419202	517.636141	18.970304	-0.051327	1.452843
279.571758	509.797408	18.975309	-0.051350	1.445242
279.485172	502.019596	18.980314	-0.051329	1.437623
279.521506	494.212692	18.985319	-0.051330	1.429954
279.414333	486.433724	18.990323	-0.051305	1.422248
279.436010	478.645238	18.995328	-0.051303	1.414512
279.299346	470.878533	19.000333	-0.051273	1.406729
278.886479	463.162687	19.005338	-0.051190	1.398907
278.977314	455.345981	19.010343	-0.051202	1.391024
279.015045	447.544019	19.015347	-0.051204	1.383102
278.777944	439.805326	19.020352	-0.051154	1.375153
278.848310	432.013441	19.025357	-0.051162	1.367155
278.733865	424.268374	19.030362	-0.051135	1.359127
278.812053	416.487120	19.035367	-0.051145	1.351046
278.815990	408.722187	19.040371	-0.051140	1.342921
278.582329	401.011162	19.045376	-0.051091	1.334762
278.653971	393.236192	19.050381	-0.051099	1.326539
278.505928	385.524615	19.055386	-0.051066	1.318293
278.301242	377.716273	19.060391	-0.051023	1.309880
278.237557	369.945064	19.065395	-0.051006	1.301479
278.155799	362.225067	19.070400	-0.050985	1.293076
278.267845	354.485803	19.075405	-0.051001	1.284632
277.832251	346.840983	19.080410	-0.050914	1.276135
278.104868	339.071558	19.085415	-0.050960	1.267575
277.921497	331.393611	19.090419	-0.050920	1.258974
277.906184	323.679167	19.095424	-0.050912	1.250304
278.019259	315.975434	19.100429	-0.050928	1.241610
277.793527	308.311985	19.105434	-0.050881	1.232835
277.554585	300.642667	19.110439	-0.050831	1.223988
277.649372	292.939190	19.115443	-0.050843	1.215103
277.559097	285.264793	19.120448	-0.050821	1.206149
277.605018	277.600599	19.125453	-0.050825	1.197168
277.385577	269.950949	19.130458	-0.050779	1.188082
277.439877	262.287993	19.135463	-0.050783	1.178966
277.269722	254.658897	19.140467	-0.050747	1.169774
277.081417	247.043378	19.145472	-0.050706	1.160521
276.916064	239.412138	19.150477	-0.050670	1.151180
276.920371	231.743442	19.155482	-0.050666	1.141752
276.764188	224.149541	19.160487	-0.050632	1.132304
276.725672	216.530132	19.165491	-0.050619	1.122770
276.831214	208.905045	19.170496	-0.050634	1.113178
276.631171	201.334595	19.175501	-0.050591	1.103506
276.500636	193.763088	19.180506	-0.050562	1.093762
276.478490	186.182325	19.185511	-0.050552	1.083942
276.233669	178.650789	19.190515	-0.050502	1.074048
276.020953	171.100601	19.195520	-0.050457	1.064043
276.042654	163.544948	19.200525	-0.050456	1.053990
275.839422	156.024739	19.205530	-0.050413	1.043836
275.651460	148.528238	19.210535	-0.050372	1.033618
275.477715	141.019274	19.215539	-0.050335	1.023284
275.382306	133.516730	19.220544	-0.050312	1.012873
274.984871	126.084872	19.225549	-0.050233	1.002378
274.419851	118.666559	19.230554	-0.050123	0.991751
274.067147	111.216956	19.235559	-0.050052	0.981016
273.282857	103.870531	19.240563	-0.049901	0.970202
272.571868	96.509724	19.245568	-0.049763	0.959264
272.408643	89.071317	19.250573	-0.049728	0.948226
271.749663	81.723800	19.255578	-0.049600	0.937065
271.060779	74.402117	19.260583	-0.049467	0.925800
270.434875	67.088328	19.265587	-0.049345	0.914425
269.794745	59.998989	19.270592	-0.049221	0.903252