Fri Mar 12 11:17:29 2021


Number of Points = 3626

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.619625	-0.165101	0.000000	-0.000060	0.716548
0.713853	-0.234299	0.005005	-0.000077	0.716444
0.476761	-0.190168	0.010010	-0.000032	0.716447
0.615420	-0.215847	0.015014	-0.000058	0.716444
0.695003	-0.231634	0.020019	-0.000072	0.716441
0.815855	-0.247167	0.025024	-0.000095	0.716452
0.579368	-0.208543	0.030029	-0.000050	0.716444
0.694292	-0.227039	0.035034	-0.000071	0.716448
0.712858	-0.230183	0.040038	-0.000075	0.716448
0.643689	-0.219196	0.045043	-0.000061	0.716444
0.662731	-0.220140	0.050048	-0.000065	0.716449
0.444940	-0.183467	0.055053	-0.000024	0.716444
0.438624	-0.181036	0.060058	-0.000022	0.716446
0.499903	-0.278557	0.065062	-0.000033	0.716274
0.616552	-0.373513	0.070067	-0.000055	0.716126
0.570833	-0.360558	0.075072	-0.000046	0.716135
0.516595	-0.354790	0.080077	-0.000036	0.716127
0.419277	-0.334888	0.085082	-0.000017	0.716132
0.659136	-0.379029	0.090086	-0.000062	0.716128
0.529304	-0.355738	0.095091	-0.000037	0.716128
0.480629	-0.466438	0.100096	-0.000028	0.715891
0.528250	-0.480429	0.105101	-0.000036	0.715879
0.528492	-0.477631	0.110106	-0.000036	0.715884
0.465517	-0.466250	0.115110	-0.000024	0.715884
0.235184	-0.426906	0.120115	0.000019	0.715880
0.533383	-0.613882	0.125120	-0.000036	0.715614
0.458186	-0.638739	0.130125	-0.000022	0.715538
0.503388	-0.645369	0.135130	-0.000030	0.715540
0.619335	-0.664208	0.140134	-0.000051	0.715543
0.415678	-0.723789	0.145139	-0.000013	0.715353
0.388398	-0.780853	0.150144	-0.000007	0.715229
0.432108	-0.790483	0.155149	-0.000015	0.715225
0.432741	-0.790905	0.160154	-0.000015	0.715224
0.392663	-0.906642	0.165158	-0.000007	0.714979
0.402681	-0.948887	0.170163	-0.000009	0.714899
0.400825	-0.944461	0.175168	-0.000008	0.714906
0.349543	-0.987105	0.180173	0.000002	0.714803
0.323440	-1.082736	0.185178	0.000007	0.714603
0.460651	-1.104384	0.190182	-0.000018	0.714608
0.138759	-1.072777	0.195187	0.000042	0.714557
0.185987	-1.220258	0.200192	0.000034	0.714280
0.223380	-1.232060	0.205197	0.000027	0.714269
0.188750	-1.239989	0.210202	0.000034	0.714240
0.201812	-1.379986	0.215206	0.000032	0.713966
0.189733	-1.380420	0.220211	0.000034	0.713961
0.298511	-1.441145	0.225216	0.000014	0.713878
0.146225	-1.531632	0.230221	0.000043	0.713644
0.137045	-1.526654	0.235226	0.000045	0.713650
0.183437	-1.628131	0.240230	0.000037	0.713464
-0.043716	-1.644043	0.245235	0.000079	0.713351
0.116763	-1.679182	0.250240	0.000050	0.713337
0.046596	-1.827511	0.255245	0.000063	0.713017
0.159188	-1.844938	0.260250	0.000042	0.713022
-0.098371	-1.897234	0.265254	0.000091	0.712826
0.036632	-1.982483	0.270259	0.000066	0.712703
0.123074	-2.040802	0.275264	0.000050	0.712617
-0.101471	-2.121534	0.280269	0.000092	0.712376
-0.501955	-2.046641	0.285274	0.000167	0.712383
-0.476665	-2.190650	0.290278	0.000163	0.712104
-0.468412	-2.202767	0.295283	0.000162	0.712082
-0.504279	-2.297956	0.300288	0.000169	0.711879
-1.006639	-2.269905	0.305293	0.000262	0.711756
-1.363135	-2.246812	0.310298	0.000329	0.711675
-2.492832	-2.155636	0.315302	0.000540	0.711455
-2.418011	-2.172170	0.320307	0.000526	0.711448
-2.486280	-2.220959	0.325312	0.000539	0.711326
-3.558236	-2.126908	0.330317	0.000739	0.711132
-3.147098	-2.197387	0.335322	0.000663	0.711137
-3.349953	-2.195259	0.340326	0.000701	0.711068
-4.305980	-2.127690	0.345331	0.000879	0.710863
-3.577842	-2.252589	0.350336	0.000744	0.710872
-4.354456	-2.118567	0.355341	0.000889	0.710862
-4.674099	-2.206502	0.360346	0.000949	0.710573
-4.978260	-2.173316	0.365350	0.001005	0.710530
-5.249759	-2.128716	0.370355	0.001056	0.710522
-4.876664	-2.197501	0.375360	0.000987	0.710517
-5.857524	-2.175886	0.380365	0.001170	0.710210
-5.848184	-2.175043	0.385370	0.001169	0.710215
-5.760601	-2.188768	0.390374	0.001153	0.710218
-6.127110	-2.127702	0.395379	0.001221	0.710209
-6.037087	-2.265036	0.400384	0.001205	0.709966
-6.985530	-2.135750	0.405389	0.001382	0.709886
-7.088409	-2.114753	0.410394	0.001401	0.709891
-6.899410	-2.147841	0.415398	0.001366	0.709891
-7.017836	-2.130164	0.420403	0.001388	0.709884
-7.408766	-2.203737	0.425408	0.001462	0.709597
-7.746414	-2.147456	0.430413	0.001525	0.709588
-7.760290	-2.143531	0.435418	0.001528	0.709591
-7.367463	-2.212712	0.440422	0.001455	0.709592
-7.924224	-2.117031	0.445427	0.001559	0.709584
-8.028249	-2.248692	0.450432	0.001578	0.709283
-8.254994	-2.223096	0.455437	0.001621	0.709253
-8.742826	-2.131660	0.460442	0.001712	0.709261
-8.177450	-2.231633	0.465446	0.001607	0.709262
-8.257915	-2.221497	0.470451	0.001622	0.709253
-8.794001	-2.248829	0.475456	0.001722	0.709007
-9.865746	-2.086856	0.480461	0.001922	0.708948
-9.327876	-2.178966	0.485466	0.001822	0.708955
-9.114287	-2.216635	0.490470	0.001783	0.708955
-9.754171	-2.105702	0.495475	0.001902	0.708949
-9.365153	-2.170816	0.500480	0.001830	0.708957
-9.713949	-2.258440	0.505485	0.001896	0.708656
-10.352173	-2.153918	0.510490	0.002015	0.708637
-10.372002	-2.148271	0.515494	0.002019	0.708641
-10.138860	-2.193283	0.520499	0.001975	0.708633
-10.033584	-2.209583	0.525504	0.001956	0.708638
-10.482346	-2.130722	0.530509	0.002040	0.708635
-10.586127	-2.237479	0.535514	0.002060	0.708383
-11.135486	-2.155372	0.540518	0.002162	0.708351
-11.442826	-2.103702	0.545523	0.002220	0.708344
-10.693288	-2.232222	0.550528	0.002081	0.708354
-10.907934	-2.198475	0.555533	0.002121	0.708344
-11.513043	-2.089291	0.560538	0.002234	0.708346
-11.336293	-2.218425	0.565542	0.002201	0.708150
-11.979049	-2.175382	0.570547	0.002321	0.708006
-11.832659	-2.197299	0.575552	0.002294	0.708014
-12.486331	-2.084870	0.580557	0.002416	0.708005
-12.427217	-2.093412	0.585562	0.002405	0.708009
-11.888673	-2.188496	0.590566	0.002305	0.708010
-12.070696	-2.158458	0.595571	0.002340	0.708005
-12.604829	-2.194463	0.600576	0.002439	0.707741
-12.917491	-2.162464	0.605581	0.002498	0.707693
-12.942792	-2.157790	0.610586	0.002503	0.707693
-12.813328	-2.177977	0.615590	0.002479	0.707698
-13.076079	-2.133743	0.620595	0.002528	0.707692
-13.031491	-2.138023	0.625600	0.002520	0.707699
-13.310019	-2.090315	0.630605	0.002572	0.707694
-13.727394	-2.165428	0.635610	0.002650	0.707394
-13.705162	-2.177472	0.640614	0.002647	0.707377
-14.541845	-2.029768	0.645619	0.002803	0.707374
-14.028059	-2.118927	0.650624	0.002707	0.707378
-13.821343	-2.158409	0.655629	0.002669	0.707372
-14.129942	-2.100827	0.660634	0.002727	0.707377
-14.042085	-2.116283	0.665638	0.002711	0.707376
-14.108951	-2.183345	0.670643	0.002724	0.707217
-14.691918	-2.147237	0.675648	0.002832	0.707081
-14.836748	-2.125999	0.680653	0.002860	0.707071
-15.210873	-2.056154	0.685658	0.002929	0.707077
-14.770656	-2.131774	0.690662	0.002848	0.707082
-14.853553	-2.121849	0.695667	0.002864	0.707072
-14.926868	-2.103562	0.700672	0.002878	0.707082
-14.870694	-2.181831	0.705677	0.002867	0.706944
-15.793644	-2.117384	0.710682	0.003040	0.706742
-15.523127	-2.162253	0.715686	0.002989	0.706749
-16.293422	-2.027268	0.720691	0.003133	0.706743
-15.636836	-2.139595	0.725696	0.003011	0.706752
-15.787605	-2.116947	0.730701	0.003040	0.706743
-16.016531	-2.075276	0.735706	0.003082	0.706744
-15.526203	-2.204363	0.740710	0.002992	0.706660
-16.780928	-2.093626	0.745715	0.003225	0.706433
-16.816553	-2.081867	0.750720	0.003232	0.706443
-16.675597	-2.110713	0.755725	0.003206	0.706435
-16.734194	-2.099326	0.760730	0.003218	0.706436
-16.824081	-2.080614	0.765734	0.003235	0.706441
-17.172065	-2.022225	0.770739	0.003300	0.706433
-16.341229	-2.164957	0.775744	0.003145	0.706443
-17.096162	-2.171888	0.780749	0.003286	0.706158
-18.009930	-2.027005	0.785754	0.003457	0.706122
-17.450319	-2.124966	0.790758	0.003353	0.706125
-17.532788	-2.114565	0.795763	0.003368	0.706116
-17.625777	-2.092932	0.800768	0.003386	0.706125
-17.481736	-2.121744	0.805773	0.003359	0.706118
-17.267548	-2.158363	0.810778	0.003320	0.706121
-17.842575	-2.166906	0.815782	0.003427	0.705897
-18.771213	-2.024213	0.820787	0.003600	0.705850
-18.301491	-2.102427	0.825792	0.003513	0.705861
-18.310308	-2.105037	0.830797	0.003515	0.705852
-18.520384	-2.064357	0.835802	0.003555	0.705858
-18.106155	-2.136792	0.840806	0.003478	0.705860
-18.495560	-2.070470	0.845811	0.003551	0.705853
-19.026265	-2.132643	0.850816	0.003650	0.705537
-19.408069	-2.074112	0.855821	0.003721	0.705518
-19.271801	-2.096610	0.860826	0.003696	0.705521
-18.989136	-2.145710	0.865830	0.003644	0.705523
-19.471485	-2.063049	0.870835	0.003734	0.705516
-19.063690	-2.130848	0.875840	0.003658	0.705525
-19.013329	-2.160258	0.880845	0.003649	0.705483
-20.217204	-2.084851	0.885850	0.003873	0.705202
-19.882623	-2.141463	0.890854	0.003811	0.705208
-20.309039	-2.069119	0.895859	0.003891	0.705200
-20.033036	-2.114203	0.900864	0.003840	0.705208
-20.280236	-2.073225	0.905869	0.003886	0.705201
-20.121376	-2.102195	0.910874	0.003857	0.705199
-20.040251	-2.134636	0.915878	0.003842	0.705162
-21.111354	-2.086935	0.920883	0.004042	0.704873
-20.629910	-2.166477	0.925888	0.003953	0.704885
-21.062963	-2.091551	0.930893	0.004034	0.704880
-21.162495	-2.073486	0.935898	0.004052	0.704880
-20.765321	-2.141144	0.940902	0.003979	0.704886
-21.144773	-2.078757	0.945907	0.004050	0.704875
-21.247792	-2.074099	0.950912	0.004069	0.704847
-22.023167	-2.067660	0.955917	0.004214	0.704581
-21.812556	-2.103996	0.960922	0.004175	0.704583
-21.928142	-2.081985	0.965926	0.004197	0.704585
-22.198405	-2.036039	0.970931	0.004247	0.704580
-21.900502	-2.085304	0.975936	0.004192	0.704587
-22.107462	-2.050605	0.980941	0.004231	0.704582
-22.152479	-2.041950	0.985946	0.004240	0.704583
-21.791800	-2.215806	0.990950	0.004173	0.704361
-22.999434	-2.054548	0.995955	0.004398	0.704252
-22.841530	-2.078857	1.000960	0.004369	0.704259
-22.918217	-2.067420	1.005965	0.004383	0.704254
-22.943865	-2.061753	1.010970	0.004388	0.704255
-22.745519	-2.096911	1.015974	0.004352	0.704255
-23.100065	-2.036943	1.020979	0.004418	0.704248
-22.920463	-2.170606	1.025984	0.004385	0.704043
-23.563853	-2.104690	1.030989	0.004505	0.703944
-24.125541	-2.003106	1.035994	0.004610	0.703946
-23.920598	-2.039634	1.040998	0.004572	0.703946
-23.820395	-2.061668	1.046003	0.004554	0.703937
-23.605461	-2.094250	1.051008	0.004514	0.703948
-23.552908	-2.105312	1.056013	0.004505	0.703944
-24.004350	-2.127350	1.061018	0.004589	0.703736
-24.669832	-2.062074	1.066022	0.004713	0.703628
-24.817204	-2.039076	1.071027	0.004741	0.703621
-24.373100	-2.113797	1.076032	0.004658	0.703629
-24.487065	-2.095401	1.081037	0.004680	0.703625
-25.070584	-1.991432	1.086042	0.004789	0.703624
-24.484695	-2.092437	1.091046	0.004680	0.703630
-24.646489	-2.134861	1.096051	0.004711	0.703486
-25.761847	-2.009342	1.101056	0.004918	0.703337
-25.526694	-2.052417	1.106061	0.004875	0.703335
-25.545683	-2.047358	1.111066	0.004879	0.703337
-25.316303	-2.086853	1.116070	0.004836	0.703340
-25.696962	-2.023303	1.121075	0.004908	0.703330
-25.597527	-2.037000	1.126080	0.004889	0.703338
-25.194237	-2.180221	1.131085	0.004815	0.703193
-26.577741	-2.029812	1.136090	0.005072	0.702998
-26.241923	-2.087281	1.141094	0.005010	0.703003
-26.460644	-2.051441	1.146099	0.005051	0.702996
-26.354733	-2.066836	1.151104	0.005032	0.703002
-26.408265	-2.061454	1.156109	0.005042	0.702993
-26.600265	-2.025432	1.161114	0.005078	0.702996
-26.392600	-2.118322	1.166118	0.005040	0.702883
-27.677836	-1.987855	1.171123	0.005279	0.702683
-26.998631	-2.105935	1.176128	0.005153	0.702688
-27.012498	-2.106272	1.181133	0.005156	0.702682
-27.547138	-2.009735	1.186138	0.005256	0.702684
-27.185606	-2.069358	1.191142	0.005189	0.702693
-27.313848	-2.052275	1.196147	0.005213	0.702681
-27.354205	-2.095703	1.201152	0.005221	0.702578
-28.591421	-1.981778	1.206157	0.005451	0.702362
-28.098149	-2.070686	1.211162	0.005360	0.702360
-27.885197	-2.103974	1.216166	0.005321	0.702368
-28.319671	-2.032864	1.221171	0.005402	0.702355
-28.369596	-2.017658	1.226176	0.005411	0.702367
-28.091621	-2.068524	1.231181	0.005360	0.702364
-28.177047	-2.065789	1.236186	0.005376	0.702338
-28.731686	-2.098502	1.241190	0.005480	0.702071
-29.057136	-2.043855	1.246195	0.005541	0.702064
-28.983790	-2.052446	1.251200	0.005527	0.702073
-28.975728	-2.055300	1.256205	0.005526	0.702069
-29.028727	-2.047807	1.261210	0.005536	0.702065
-28.834776	-2.079176	1.266214	0.005500	0.702070
-29.074557	-2.075267	1.271219	0.005545	0.701991
-29.762823	-2.076406	1.276224	0.005674	0.701740
-29.610489	-2.106528	1.281229	0.005646	0.701734
-30.120253	-2.014037	1.286234	0.005741	0.701736
-30.041273	-2.024715	1.291238	0.005726	0.701743
-29.867602	-2.060068	1.296243	0.005694	0.701733
-29.672604	-2.090354	1.301248	0.005658	0.701742
-30.166853	-2.048801	1.306253	0.005751	0.701647
-31.195588	-1.973470	1.311258	0.005943	0.701427
-30.189868	-2.150214	1.316262	0.005756	0.701432
-30.743700	-2.055107	1.321267	0.005859	0.701424
-31.097292	-1.986838	1.326272	0.005925	0.701434
-30.864854	-2.031706	1.331277	0.005882	0.701427
-30.887574	-2.026448	1.336282	0.005887	0.701429
-30.858199	-2.047096	1.341286	0.005882	0.701397
-31.596648	-2.055509	1.346291	0.006019	0.701112
-31.700219	-2.034216	1.351296	0.006039	0.701118
-31.991159	-1.985444	1.356301	0.006093	0.701111
-31.699455	-2.035793	1.361306	0.006039	0.701114
-31.230284	-2.115707	1.366310	0.005952	0.701121
-31.791914	-2.021286	1.371315	0.006057	0.701108
-31.665415	-2.047608	1.376320	0.006034	0.701100
-31.774480	-2.142846	1.381325	0.006055	0.700867
-32.157314	-2.076183	1.386330	0.006126	0.700864
-32.385776	-2.031271	1.391334	0.006169	0.700871
-32.341981	-2.042150	1.396339	0.006161	0.700865
-31.929770	-2.113296	1.401344	0.006085	0.700869
-32.268594	-2.055021	1.406349	0.006148	0.700864
-33.018421	-2.078231	1.411354	0.006288	0.700545
-32.909491	-2.105615	1.416358	0.006268	0.700529
-33.185406	-2.060557	1.421363	0.006320	0.700520
-32.915432	-2.103607	1.426368	0.006270	0.700529
-33.313154	-2.034903	1.431373	0.006344	0.700524
-33.166645	-2.059632	1.436378	0.006317	0.700527
-32.797359	-2.202124	1.441382	0.006249	0.700371
-34.369110	-2.001373	1.446387	0.006541	0.700209
-33.853608	-2.090521	1.451392	0.006446	0.700214
-33.940584	-2.076307	1.456397	0.006462	0.700211
-34.272894	-2.017495	1.461402	0.006524	0.700209
-33.708291	-2.113783	1.466406	0.006420	0.700217
-34.121849	-2.043445	1.471411	0.006497	0.700210
-34.652637	-2.081824	1.476416	0.006596	0.699940
-34.867474	-2.069310	1.481421	0.006636	0.699887
-35.024616	-2.042119	1.486426	0.006666	0.699884
-34.765700	-2.084473	1.491430	0.006618	0.699892
-35.200644	-2.011895	1.496435	0.006699	0.699881
-34.819353	-2.073881	1.501440	0.006629	0.699892
-34.677061	-2.100552	1.506445	0.006602	0.699889
-35.776001	-2.050576	1.511450	0.006807	0.699592
-35.849697	-2.033807	1.516454	0.006821	0.699599
-35.957524	-2.018447	1.521459	0.006842	0.699591
-35.820909	-2.040339	1.526464	0.006816	0.699595
-35.585509	-2.083923	1.531469	0.006773	0.699591
-35.841502	-2.038295	1.536474	0.006821	0.699591
-35.653772	-2.069955	1.541478	0.006786	0.699594
-36.422329	-2.099084	1.546483	0.006930	0.699256
-36.491697	-2.081858	1.551488	0.006943	0.699265
-36.715952	-2.045540	1.556493	0.006985	0.699257
-36.744087	-2.038550	1.561498	0.006990	0.699261
-36.550560	-2.072168	1.566502	0.006955	0.699262
-36.707275	-2.047243	1.571507	0.006984	0.699255
-36.575686	-2.099826	1.576512	0.006960	0.699195
-37.393923	-2.072673	1.581517	0.007113	0.698953
-37.217167	-2.105337	1.586522	0.007080	0.698951
-37.601784	-2.034500	1.591526	0.007152	0.698955
-37.892515	-1.985479	1.596531	0.007206	0.698948
-37.534650	-2.045872	1.601536	0.007140	0.698955
-37.444545	-2.063505	1.606541	0.007123	0.698951
-37.828808	-2.020847	1.611546	0.007195	0.698898
-38.210684	-2.080063	1.616550	0.007267	0.698638
-38.366333	-2.054593	1.621555	0.007296	0.698633
-38.634220	-2.003424	1.626560	0.007346	0.698639
-38.524542	-2.023663	1.631565	0.007326	0.698638
-38.482256	-2.033496	1.636570	0.007318	0.698632
-38.340896	-2.054357	1.641574	0.007292	0.698641
-38.726859	-1.989883	1.646579	0.007365	0.698631
-38.759186	-2.121599	1.651584	0.007371	0.698351
-38.948572	-2.090341	1.656589	0.007406	0.698345
-39.646744	-1.964960	1.661594	0.007537	0.698346
-38.869252	-2.099243	1.666598	0.007392	0.698355
-39.034798	-2.075153	1.671603	0.007423	0.698343
-39.163930	-2.048924	1.676608	0.007448	0.698349
-39.183574	-2.128904	1.681613	0.007452	0.698179
-40.317919	-2.012232	1.686618	0.007663	0.698004
-39.686755	-2.120882	1.691622	0.007546	0.698011
-40.316869	-2.013046	1.696627	0.007664	0.698001
-40.164578	-2.035362	1.701632	0.007636	0.698011
-39.662025	-2.126481	1.706637	0.007542	0.698007
-40.204541	-2.030817	1.711642	0.007644	0.698004
-40.346297	-2.127242	1.716646	0.007670	0.697756
-40.989719	-2.045439	1.721651	0.007790	0.697688
-41.020497	-2.034070	1.726656	0.007796	0.697700
-40.990345	-2.042847	1.731661	0.007791	0.697692
-41.049738	-2.033122	1.736666	0.007802	0.697690
-40.957195	-2.045475	1.741670	0.007785	0.697698
-41.357081	-1.977778	1.746675	0.007860	0.697690
-41.351402	-2.090363	1.751680	0.007859	0.697462
-41.777228	-2.059042	1.756685	0.007939	0.697371
-41.806577	-2.055250	1.761690	0.007945	0.697367
-41.633859	-2.081216	1.766694	0.007913	0.697376
-41.930770	-2.033072	1.771699	0.007968	0.697366
-41.742352	-2.062796	1.776704	0.007934	0.697373
-42.069951	-2.004311	1.781709	0.007995	0.697373
-42.398010	-2.070797	1.786714	0.008056	0.697118
-42.340940	-2.098201	1.791718	0.008046	0.697082
-42.819734	-2.017610	1.796723	0.008135	0.697072
-42.773586	-2.021538	1.801728	0.008127	0.697080
-42.350131	-2.097823	1.806733	0.008049	0.697078
-42.819023	-2.015207	1.811738	0.008136	0.697075
-42.891476	-2.001772	1.816742	0.008150	0.697076
-43.144834	-2.119659	1.821747	0.008198	0.696743
-43.172213	-2.111699	1.826752	0.008203	0.696748
-43.694556	-2.019853	1.831757	0.008300	0.696745
-43.707364	-2.018818	1.836762	0.008303	0.696742
-43.192894	-2.104984	1.841766	0.008208	0.696753
-43.665857	-2.025276	1.846771	0.008296	0.696743
-43.551539	-2.091324	1.851776	0.008275	0.696649
-44.138807	-2.087672	1.856781	0.008385	0.696442
-44.362206	-2.048841	1.861786	0.008427	0.696440
-44.587513	-2.005461	1.866790	0.008469	0.696446
-44.273919	-2.065405	1.871795	0.008411	0.696437
-44.149838	-2.083736	1.876800	0.008388	0.696444
-44.481972	-2.024591	1.881805	0.008450	0.696443
-44.700982	-2.066129	1.886810	0.008491	0.696278
-44.859800	-2.108362	1.891814	0.008521	0.696134
-45.228286	-2.048354	1.896819	0.008590	0.696121
-45.098886	-2.067101	1.901824	0.008566	0.696130
-45.075853	-2.072382	1.906829	0.008562	0.696127
-45.238027	-2.044319	1.911834	0.008593	0.696124
-45.312142	-2.027680	1.916838	0.008607	0.696131
-45.454263	-2.109508	1.921843	0.008633	0.695911
-45.543836	-2.111410	1.926848	0.008650	0.695874
-45.980405	-2.034665	1.931853	0.008732	0.695872
-46.156698	-2.003471	1.936858	0.008765	0.695870
-45.437599	-2.129020	1.941862	0.008632	0.695875
-45.889468	-2.052298	1.946867	0.008716	0.695867
-46.125284	-2.111025	1.951872	0.008760	0.695661
-47.025424	-2.012502	1.956877	0.008928	0.695533
-46.705569	-2.070273	1.961882	0.008869	0.695531
-46.557293	-2.092889	1.966886	0.008841	0.695538
-47.003883	-2.016073	1.971891	0.008925	0.695532
-46.752653	-2.059730	1.976896	0.008878	0.695534
-46.767142	-2.057284	1.981901	0.008881	0.695533
-47.457859	-2.071060	1.986906	0.009010	0.695253
-47.246022	-2.120869	1.991910	0.008971	0.695227
-47.660556	-2.052443	1.996915	0.009049	0.695216
-47.771720	-2.028616	2.001920	0.009070	0.695223
-47.614608	-2.056158	2.011917	0.009041	0.695223
-47.699123	-2.084307	2.021914	0.009057	0.695134
-48.489376	-2.059150	2.031910	0.009205	0.694896
-48.419123	-2.070318	2.041907	0.009193	0.694897
-48.666077	-2.025776	2.051904	0.009239	0.694897
-48.525040	-2.050947	2.061901	0.009213	0.694896
-48.019478	-1.997538	2.071898	0.009120	0.695188
-47.804254	-2.089289	2.081894	0.009080	0.695078
-47.294958	-2.109983	2.091891	0.008986	0.695220
-47.480067	-2.075710	2.101888	0.009021	0.695222
-47.482161	-2.075577	2.111885	0.009022	0.695220
-47.568417	-2.061501	2.121882	0.009039	0.695216
-47.579256	-2.058584	2.131878	0.009041	0.695217
-47.611474	-2.052045	2.141875	0.009048	0.695218
-47.623445	-2.048085	2.151872	0.009051	0.695220
-47.095771	-2.039371	2.161869	0.008953	0.695429
-47.042223	-1.999350	2.171866	0.008944	0.695529
-46.814195	-2.039504	2.181862	0.008902	0.695529
-46.576939	-2.079850	2.191859	0.008858	0.695532
-46.661511	-2.020348	2.201856	0.008875	0.695622
-45.703885	-2.069395	2.211853	0.008697	0.695869
-46.007987	-2.014815	2.221850	0.008754	0.695869
-45.827158	-2.047084	2.231846	0.008721	0.695868
-45.695416	-2.045368	2.241843	0.008697	0.695918
-45.009867	-2.066275	2.251840	0.008570	0.696124
-45.154819	-2.040124	2.261837	0.008598	0.696123
-45.069469	-2.055323	2.271834	0.008582	0.696122
-44.823745	-2.032408	2.281830	0.008537	0.696257
-44.016117	-2.087721	2.291827	0.008387	0.696437
-44.341912	-2.025940	2.301824	0.008449	0.696443
-44.202475	-2.051208	2.311821	0.008423	0.696441
-43.972920	-1.956234	2.321818	0.008381	0.696717
-43.435553	-2.037573	2.331814	0.008282	0.696746
-43.401166	-2.042876	2.341811	0.008276	0.696746
-42.943605	-2.031573	2.351808	0.008191	0.696935
-42.546318	-2.031698	2.361805	0.008118	0.697078
-42.660526	-2.011493	2.371802	0.008140	0.697076
-42.584288	-2.006810	2.381798	0.008126	0.697112
-41.868089	-2.006443	2.391795	0.007993	0.697372
-41.709211	-2.034604	2.401792	0.007964	0.697371
-41.660888	-2.043658	2.411789	0.007956	0.697369
-41.410367	-1.971233	2.421786	0.007910	0.697607
-40.772108	-2.042520	2.431782	0.007792	0.697692
-41.044760	-1.993058	2.441779	0.007843	0.697693
-40.788341	-1.975500	2.451776	0.007796	0.697820
-39.799088	-2.057609	2.461773	0.007612	0.698011
-39.845468	-2.049926	2.471770	0.007621	0.698009
-39.997987	-2.022276	2.481766	0.007650	0.698009
-39.221674	-2.030607	2.491763	0.007506	0.698272
-38.866362	-2.057837	2.501760	0.007441	0.698345
-38.879072	-2.054316	2.511757	0.007444	0.698346
-38.909763	-2.047550	2.521754	0.007450	0.698347
-38.141615	-2.044322	2.531750	0.007308	0.698631
-38.274986	-2.018128	2.541747	0.007333	0.698635
-37.940490	-2.076801	2.551744	0.007271	0.698636
-37.828189	-2.018259	2.561741	0.007251	0.698795
-37.171664	-2.058031	2.571738	0.007129	0.698951
-37.375492	-2.023077	2.581734	0.007168	0.698947
-37.309560	-2.030736	2.591731	0.007156	0.698954
-36.297445	-2.058496	2.601728	0.006968	0.699263
-36.441579	-2.034037	2.611725	0.006996	0.699259
-36.423114	-2.035767	2.621722	0.006993	0.699261
-36.054667	-2.021526	2.631718	0.006925	0.699423
-35.559218	-2.024332	2.641715	0.006833	0.699595
-35.506473	-2.033869	2.651712	0.006824	0.699594
-35.520051	-2.031771	2.661709	0.006827	0.699592
-34.609372	-2.049068	2.671706	0.006658	0.699885
-34.686544	-2.033588	2.681702	0.006673	0.699888
-34.562170	-2.055245	2.691699	0.006650	0.699888
-34.314681	-2.025133	2.701696	0.006605	0.700037
-33.645479	-2.057803	2.711693	0.006481	0.700212
-33.804178	-2.029479	2.721690	0.006511	0.700211
-33.855832	-2.019667	2.731686	0.006521	0.700211
-33.018665	-2.017277	2.741683	0.006366	0.700517
-32.957754	-2.021871	2.751680	0.006355	0.700529
-32.732213	-2.061607	2.761677	0.006314	0.700529
-32.551221	-2.020528	2.771674	0.006281	0.700676
-31.814173	-2.059925	2.781670	0.006144	0.700861
-32.088303	-2.007856	2.791667	0.006196	0.700867
-31.837869	-2.051104	2.801664	0.006150	0.700868
-31.533530	-1.999961	2.811661	0.006094	0.701081
-31.410775	-2.005238	2.821658	0.006071	0.701113
-31.298020	-2.023780	2.831654	0.006051	0.701115
-30.759505	-2.018910	2.841651	0.005951	0.701319
-30.324933	-2.040527	2.851648	0.005871	0.701431
-30.255895	-2.051118	2.861645	0.005859	0.701433
-30.263200	-2.019875	2.871642	0.005861	0.701492
-29.772791	-1.986016	2.881638	0.005770	0.701737
-29.432227	-2.045409	2.891635	0.005707	0.701738
-29.440024	-2.042259	2.901632	0.005709	0.701741
-28.895607	-1.996039	2.911629	0.005608	0.702030
-28.478060	-2.051229	2.921626	0.005531	0.702067
-28.703239	-2.011172	2.931622	0.005574	0.702066
-28.474410	-1.993719	2.941619	0.005532	0.702183
-27.702805	-2.039522	2.951616	0.005389	0.702367
-27.750018	-2.030039	2.961613	0.005398	0.702368
-27.759780	-2.028664	2.971610	0.005400	0.702366
-27.040051	-1.997825	2.981606	0.005267	0.702687
-26.729894	-2.051907	2.991603	0.005210	0.702688
-26.826863	-2.034868	3.001600	0.005228	0.702687
-26.468418	-2.029600	3.011597	0.005162	0.702825
-25.823963	-2.057437	3.021594	0.005043	0.703000
-26.307443	-1.971793	3.031590	0.005133	0.702998
-25.764221	-2.067700	3.041587	0.005033	0.702998
-25.307697	-1.990628	3.051584	0.004948	0.703317
-25.215227	-1.995752	3.061581	0.004932	0.703339
-25.032551	-2.030161	3.071578	0.004898	0.703334
-24.975028	-1.970823	3.081574	0.004888	0.703474
-24.123757	-2.044625	3.091571	0.004730	0.703630
-24.206248	-2.028619	3.101568	0.004746	0.703631
-24.267711	-2.011987	3.111565	0.004758	0.703642
-23.353067	-2.021941	3.121562	0.004589	0.703949
-23.389888	-2.016713	3.131558	0.004596	0.703946
-23.129233	-2.061692	3.141555	0.004548	0.703947
-23.122888	-1.995027	3.151552	0.004547	0.704083
-22.401339	-2.037328	3.161549	0.004414	0.704256
-22.602255	-2.000403	3.171546	0.004452	0.704257
-22.447640	-2.028492	3.181542	0.004424	0.704255
-21.773042	-1.985770	3.191539	0.004298	0.704582
-21.675553	-1.997236	3.201536	0.004281	0.704593
-21.414186	-2.043231	3.211533	0.004233	0.704593
-21.283833	-1.990502	3.221530	0.004209	0.704745
-20.618927	-2.038990	3.231526	0.004086	0.704885
-20.696428	-2.023796	3.241523	0.004101	0.704887
-20.592217	-2.040959	3.251520	0.004082	0.704888
-19.775291	-2.048839	3.261517	0.003931	0.705165
-19.973316	-1.991236	3.271514	0.003968	0.705208
-19.792475	-2.023146	3.281510	0.003935	0.705208
-19.735436	-1.976264	3.291507	0.003925	0.705322
-18.724392	-2.054158	3.301504	0.003737	0.705526
-18.716937	-2.055314	3.311501	0.003737	0.705526
-18.996051	-2.006082	3.321498	0.003789	0.705523
-18.138159	-2.038031	3.331494	0.003630	0.705766
-17.820886	-2.045613	3.341491	0.003571	0.705863
-17.942829	-2.024324	3.351488	0.003595	0.705861
-17.789904	-2.050945	3.361485	0.003567	0.705861
-17.325352	-2.005405	3.371482	0.003481	0.706118
-16.901536	-2.078254	3.381478	0.003403	0.706123
-17.049062	-2.050345	3.391475	0.003431	0.706125
-16.751706	-2.036270	3.401472	0.003376	0.706258
-16.087596	-2.062357	3.411469	0.003253	0.706443
-16.227130	-2.038595	3.421466	0.003279	0.706439
-16.044176	-2.070995	3.431462	0.003246	0.706439
-15.635153	-2.010191	3.441459	0.003170	0.706706
-15.351673	-2.038527	3.451456	0.003118	0.706750
-15.315250	-2.044808	3.461453	0.003112	0.706749
-15.291331	-1.976481	3.471450	0.003108	0.706894
-14.392929	-2.046380	3.481446	0.002941	0.707074
-14.480594	-2.028674	3.491443	0.002958	0.707077
-14.477924	-2.022943	3.501440	0.002958	0.707088
-13.572232	-2.041385	3.511437	0.002790	0.707374
-13.810951	-1.999129	3.521434	0.002835	0.707372
-13.549481	-2.045874	3.531430	0.002787	0.707371
-13.381402	-1.980348	3.541427	0.002756	0.707561
-12.314888	-2.102911	3.551424	0.002559	0.707696
-12.342070	-2.095517	3.561421	0.002564	0.707700
-12.338023	-2.096261	3.571418	0.002564	0.707698
-11.615966	-2.125218	3.581414	0.002430	0.707897
-11.482893	-2.092791	3.591411	0.002406	0.708009
-11.194459	-2.142235	3.601408	0.002353	0.708011
-11.508593	-2.085566	3.611405	0.002412	0.708012
-11.118648	-2.055749	3.621402	0.002340	0.708210
-10.405675	-2.114445	3.631398	0.002208	0.708346
-10.659335	-2.068010	3.641395	0.002256	0.708347
-10.467130	-2.101510	3.651392	0.002220	0.708347
-10.050956	-2.053961	3.661389	0.002143	0.708590
-9.847410	-2.066540	3.671386	0.002106	0.708636
-9.835549	-2.068326	3.681382	0.002105	0.708636
-9.642324	-2.041836	3.691379	0.002069	0.708757
-8.821384	-2.088409	3.701376	0.001917	0.708955
-9.076279	-2.042418	3.711373	0.001965	0.708955
-8.888779	-2.076796	3.721370	0.001931	0.708952
-7.875957	-2.111963	3.731366	0.001743	0.709242
-7.787326	-2.118019	3.741363	0.001727	0.709260
-7.395983	-2.186890	3.751360	0.001654	0.709261
-7.595116	-2.149823	3.761357	0.001692	0.709263
-6.905311	-2.139893	3.771354	0.001564	0.709528
-6.888846	-2.110578	3.781350	0.001562	0.709591
-6.479881	-2.183330	3.791347	0.001486	0.709590
-6.491757	-2.178464	3.801344	0.001489	0.709595
-6.278119	-2.111436	3.811341	0.001450	0.709804
-5.765083	-2.159463	3.821338	0.001355	0.709889
-5.826340	-2.150095	3.831334	0.001367	0.709885
-5.789662	-2.154193	3.841331	0.001361	0.709889
-4.933529	-2.148160	3.851328	0.001202	0.710205
-4.962958	-2.136644	3.861325	0.001208	0.710216
-4.752069	-2.173939	3.871322	0.001169	0.710216
-5.062643	-2.083063	3.881318	0.001228	0.710286
-3.902598	-2.166781	3.891315	0.001012	0.710530
-4.035214	-2.141060	3.901312	0.001037	0.710533
-4.018301	-2.143434	3.911309	0.001035	0.710533
-3.434953	-2.148914	3.921306	0.000927	0.710729
-3.253403	-2.112516	3.931302	0.000894	0.710865
-2.962324	-2.161985	3.941299	0.000840	0.710869
-2.987434	-2.157067	3.951296	0.000845	0.710868
-2.294750	-2.162790	3.961293	0.000717	0.711102
-2.272814	-2.149572	3.971290	0.000713	0.711135
-2.314759	-2.141105	3.981286	0.000722	0.711136
-2.139970	-2.126649	3.991283	0.000690	0.711226
-1.997835	-2.037965	4.001280	0.000664	0.711452
-1.970852	-2.041311	4.011277	0.000659	0.711454
-1.907529	-1.979814	4.021274	0.000648	0.711598
-1.496115	-1.973549	4.031270	0.000572	0.711756
-1.477920	-1.974779	4.041267	0.000569	0.711759
-1.390653	-1.845723	4.051264	0.000554	0.712046
-1.089129	-1.876301	4.061261	0.000498	0.712091
-1.228641	-1.783852	4.071258	0.000525	0.712224
-1.024989	-1.739983	4.081254	0.000487	0.712383
-0.862839	-1.714129	4.091251	0.000458	0.712491
-0.697127	-1.636072	4.101248	0.000427	0.712704
-0.789178	-1.562230	4.111245	0.000445	0.712817
-0.575115	-1.499963	4.121242	0.000406	0.713016
-0.723975	-1.383729	4.131238	0.000434	0.713193
-0.735277	-1.301921	4.141235	0.000437	0.713351
-0.558582	-1.198926	4.151232	0.000404	0.713617
-0.622897	-1.112265	4.161229	0.000417	0.713766
-0.421900	-1.046395	4.171226	0.000380	0.713967
-0.607983	-0.875110	4.181222	0.000415	0.714240
-0.450501	-0.794966	4.191219	0.000386	0.714454
-0.344968	-0.702346	4.201216	0.000367	0.714674
-0.256355	-0.601874	4.211213	0.000351	0.714904
-0.217874	-0.448279	4.221210	0.000344	0.715221
-0.193538	-0.328977	4.231206	0.000340	0.715465
-0.116188	-0.202521	4.241203	0.000326	0.715742
-0.040822	-0.087961	4.251200	0.000313	0.715995
0.000000	0.051327	4.261197	0.000306	0.716284
0.006506	0.679322	4.266202	0.000304	0.717529
0.239095	1.898370	4.271206	0.000261	0.720017
0.470010	3.704362	4.276211	0.000217	0.723647
0.733527	6.048655	4.281216	0.000166	0.728320
1.231000	8.879056	4.286221	0.000072	0.733985
1.630834	12.193596	4.291226	-0.000004	0.740500
1.924903	15.979398	4.296230	-0.000061	0.747818
2.532562	20.131200	4.301235	-0.000176	0.755857
2.997049	24.685935	4.306240	-0.000266	0.764512
3.325598	29.649771	4.311245	-0.000330	0.773776
3.790422	34.924792	4.316250	-0.000419	0.783538
4.363698	40.504911	4.321254	-0.000530	0.793759
5.075069	46.366242	4.326259	-0.000666	0.804389
5.535379	52.560680	4.331264	-0.000755	0.815383
6.047425	58.999820	4.336269	-0.000854	0.826666
6.915541	65.640657	4.341274	-0.001020	0.838245
7.378089	72.547451	4.346278	-0.001110	0.849990
8.547836	79.554305	4.351283	-0.001332	0.861945
9.444358	86.808686	4.356288	-0.001504	0.874059
9.802971	94.325588	4.361293	-0.001575	0.886276
12.994645	101.523612	4.366298	-0.002174	0.898609
13.766094	109.323062	4.371302	-0.002322	0.911048
14.373973	117.269968	4.376307	-0.002440	0.923501
15.325994	125.272446	4.381312	-0.002622	0.935964
16.146221	133.404314	4.386317	-0.002780	0.948422
16.999115	141.619927	4.391322	-0.002944	0.960850
23.493323	148.974752	4.396326	-0.004158	0.973298
24.502340	157.446600	4.401331	-0.004351	0.985817
25.043717	166.040072	4.406336	-0.004457	0.998236
25.522731	174.660102	4.411341	-0.004552	1.010524
26.186374	183.271738	4.416346	-0.004680	1.022697
26.820542	191.917688	4.421350	-0.004804	1.034766
27.803094	200.527428	4.426355	-0.004992	1.046728
28.608266	209.187092	4.431360	-0.005147	1.058581
29.273045	217.896495	4.436365	-0.005277	1.070335
30.367135	226.528065	4.441370	-0.005486	1.081957
31.134370	235.227663	4.446374	-0.005634	1.093469
32.552490	243.835264	4.451379	-0.005903	1.104887
33.862529	252.459686	4.456384	-0.006152	1.116185
34.493042	261.177805	4.461389	-0.006275	1.127340
35.413988	269.852444	4.466394	-0.006452	1.138393
36.437627	278.504894	4.471398	-0.006648	1.149334
37.417508	287.173509	4.476403	-0.006836	1.160182
38.227786	295.819862	4.481408	-0.006992	1.170867
39.021711	304.466889	4.486413	-0.007145	1.181452
39.841481	313.107978	4.491418	-0.007303	1.191941
40.517422	321.724014	4.496422	-0.007434	1.202279
41.903081	330.239680	4.501427	-0.007698	1.212553
42.705045	338.834243	4.506432	-0.007852	1.222717
43.499259	347.447542	4.511437	-0.008005	1.232816
44.335095	356.001676	4.516442	-0.008166	1.242773
45.377643	364.520312	4.521446	-0.008366	1.252650
46.011738	373.095341	4.526451	-0.008489	1.262436
46.529916	381.665640	4.531456	-0.008591	1.272118
47.210072	390.179585	4.536461	-0.008723	1.281695
47.801772	398.704099	4.541466	-0.008838	1.291196
48.561443	407.170204	4.546470	-0.008985	1.300594
49.610009	415.650019	4.551475	-0.009185	1.309992
50.497981	424.149636	4.556480	-0.009356	1.319315
51.304585	432.563839	4.561485	-0.009511	1.328467
51.879004	441.027409	4.566490	-0.009624	1.337566
53.113138	449.336187	4.571494	-0.009858	1.346557
53.816069	457.777587	4.576499	-0.009995	1.355534
54.049572	466.233701	4.581504	-0.010043	1.364385
54.489299	474.667313	4.586509	-0.010130	1.373192
55.262778	483.023931	4.591514	-0.010279	1.381920
55.497785	491.465843	4.596518	-0.010328	1.390588
56.001460	499.851440	4.601523	-0.010427	1.399191
56.985965	508.126863	4.606528	-0.010616	1.407711
58.044073	516.424116	4.611533	-0.010818	1.416213
58.678079	524.772904	4.616538	-0.010941	1.424645
58.892178	533.184450	4.621542	-0.010986	1.433021
59.758287	541.454128	4.626547	-0.011153	1.441314
60.468857	549.749927	4.631552	-0.011290	1.449560
60.918806	558.099933	4.636557	-0.011379	1.457770
61.839066	566.349078	4.641562	-0.011555	1.465911
62.242205	574.736708	4.646566	-0.011636	1.474058
62.980286	583.002343	4.651571	-0.011778	1.482097
63.689936	591.260588	4.656576	-0.011915	1.490080
64.162705	599.566183	4.661581	-0.012008	1.498028
64.964186	607.805013	4.666586	-0.012163	1.505922
65.446900	616.102431	4.671590	-0.012258	1.513781
66.319463	624.324511	4.676595	-0.012425	1.521588
66.566835	632.639230	4.681600	-0.012477	1.529346
66.936611	640.929245	4.686605	-0.012550	1.537061
67.775215	649.131423	4.691610	-0.012712	1.544726
68.372662	657.393284	4.696614	-0.012828	1.552372
68.896608	665.653375	4.701619	-0.012931	1.559967
69.118375	673.923098	4.706624	-0.012977	1.567491
69.562219	682.177942	4.711629	-0.013065	1.574997
69.983231	690.414869	4.716634	-0.013148	1.582448
70.230051	698.675939	4.721638	-0.013199	1.589860
70.922597	706.876949	4.726643	-0.013333	1.597248
71.381641	715.081605	4.731648	-0.013424	1.604572
71.803405	723.307036	4.736653	-0.013507	1.611876
72.556654	731.486153	4.741658	-0.013653	1.619152
72.791685	739.726549	4.746662	-0.013702	1.626377
73.259035	748.000988	4.751667	-0.013794	1.633632
73.777736	756.163528	4.756672	-0.013895	1.640764
74.242678	764.349525	4.761677	-0.013987	1.647879
74.752849	772.546380	4.766682	-0.014087	1.654978
75.554383	780.673718	4.771686	-0.014241	1.662027
76.112340	788.870552	4.776691	-0.014350	1.669072
76.617409	797.060803	4.781696	-0.014449	1.676074
76.811524	805.280978	4.786701	-0.014490	1.683031
77.426202	813.439819	4.791706	-0.014610	1.689964
77.906155	821.628703	4.796710	-0.014704	1.696875
78.383211	829.814416	4.801715	-0.014798	1.703755
78.883990	837.996452	4.806720	-0.014896	1.710607
79.617639	846.144720	4.811725	-0.015038	1.717435
80.223624	854.292867	4.816730	-0.015156	1.724218
80.494583	862.479040	4.821734	-0.015211	1.730963
80.931129	870.683751	4.826739	-0.015298	1.737717
81.380201	878.837175	4.831744	-0.015386	1.744405
81.823906	887.011636	4.836749	-0.015474	1.751084
82.169620	895.211586	4.841754	-0.015543	1.757746
82.517727	903.358233	4.846758	-0.015613	1.764340
82.969647	911.528736	4.851763	-0.015702	1.770941
83.974954	919.622528	4.856768	-0.015895	1.777525
84.706893	927.742825	4.861773	-0.016036	1.784072
85.005639	935.969228	4.866778	-0.016097	1.790625
85.429898	944.151354	4.871782	-0.016181	1.797135
86.184921	952.240990	4.876787	-0.016326	1.803588
86.644701	960.377668	4.881792	-0.016417	1.810020
86.683606	968.588722	4.886797	-0.016429	1.816436
87.103542	976.724287	4.891802	-0.016512	1.822816
87.483522	984.868315	4.896806	-0.016588	1.829175
88.148094	992.990005	4.901811	-0.016717	1.835530
88.583151	1001.112997	4.906816	-0.016803	1.841835
89.072797	1009.238560	4.911821	-0.016899	1.848128
89.714292	1017.385182	4.916826	-0.017024	1.854433
90.081383	1025.516178	4.921830	-0.017097	1.860672
90.324057	1033.699610	4.926835	-0.017147	1.866916
90.674158	1041.864133	4.931840	-0.017217	1.873137
90.950860	1050.005580	4.936845	-0.017274	1.879312
91.401520	1058.109337	4.941850	-0.017363	1.885458
91.836372	1066.227558	4.946854	-0.017449	1.891592
92.265208	1074.361324	4.951859	-0.017534	1.897718
92.885481	1082.439420	4.956864	-0.017654	1.903804
93.217092	1090.585341	4.961869	-0.017721	1.909888
93.650307	1098.723806	4.966874	-0.017806	1.915959
93.824624	1106.858289	4.971878	-0.017844	1.921979
94.325248	1114.966671	4.976883	-0.017942	1.927997
94.672178	1123.112912	4.981888	-0.018012	1.934006
95.228115	1131.201805	4.986893	-0.018120	1.939978
95.394096	1139.356700	4.991898	-0.018156	1.945937
95.636588	1147.520969	4.996902	-0.018206	1.951893
96.003185	1155.654452	5.001907	-0.018280	1.957822
96.336644	1163.730824	5.006912	-0.018347	1.963688
96.892321	1171.802557	5.011917	-0.018455	1.969557
97.330757	1179.918320	5.016922	-0.018542	1.975428
97.598908	1188.021508	5.021926	-0.018597	1.981253
97.802767	1196.160776	5.026931	-0.018640	1.987081
98.188148	1204.271859	5.031936	-0.018716	1.992891
98.607534	1212.356713	5.036941	-0.018799	1.998668
98.834694	1220.474159	5.041946	-0.018847	2.004432
98.866175	1228.615114	5.046950	-0.018858	2.010175
99.242742	1236.722130	5.051955	-0.018933	2.015914
99.417181	1244.820000	5.056960	-0.018970	2.021609
99.949894	1252.882646	5.061965	-0.019074	2.027300
100.372841	1261.022467	5.066970	-0.019158	2.033018
100.680141	1269.110162	5.071974	-0.019220	2.038672
101.147384	1277.189631	5.076979	-0.019312	2.044320
101.587638	1285.266857	5.081984	-0.019399	2.049949
101.771995	1293.405283	5.086989	-0.019439	2.055578
102.123657	1301.501914	5.091994	-0.019509	2.061180
102.278667	1309.604242	5.096998	-0.019543	2.066751
102.777253	1317.712944	5.102003	-0.019641	2.072345
102.974399	1325.816392	5.107008	-0.019682	2.077891
103.159949	1333.915311	5.112013	-0.019722	2.083418
103.766696	1341.965688	5.117018	-0.019840	2.088939
104.218935	1350.057968	5.122022	-0.019929	2.094458
104.539451	1358.155384	5.127027	-0.019994	2.099953
104.801353	1366.249314	5.132032	-0.020047	2.105425
105.405557	1374.335761	5.137037	-0.020165	2.110912
105.775865	1382.490570	5.142042	-0.020239	2.116407
106.059099	1390.552797	5.147046	-0.020297	2.121818
106.386711	1398.641883	5.152051	-0.020363	2.127237
106.594901	1406.746916	5.157056	-0.020406	2.132641
106.868609	1414.826953	5.162061	-0.020462	2.138021
107.414346	1422.873662	5.167066	-0.020569	2.143392
107.695349	1430.963478	5.172070	-0.020626	2.148752
108.227579	1439.070355	5.177075	-0.020730	2.154134
108.687618	1447.134852	5.182080	-0.020821	2.159467
109.022177	1455.205775	5.187085	-0.020888	2.164780
109.065767	1463.354505	5.192090	-0.020901	2.170104
109.367611	1471.433046	5.197094	-0.020962	2.175392
109.907003	1479.492455	5.202099	-0.021068	2.180678
110.072500	1487.592538	5.207104	-0.021104	2.185942
110.335453	1495.698964	5.212109	-0.021158	2.191207
111.184185	1503.733043	5.217114	-0.021321	2.196465
111.578372	1511.775901	5.222118	-0.021399	2.201676
111.909347	1519.873324	5.227123	-0.021465	2.206903
112.366913	1527.942594	5.232128	-0.021556	2.212111
112.967742	1535.999581	5.237133	-0.021672	2.217312
113.089824	1544.132869	5.242138	-0.021700	2.222506
113.179965	1552.228317	5.247142	-0.021722	2.227661
113.552164	1560.336845	5.252147	-0.021796	2.232838
113.897977	1568.386673	5.257152	-0.021866	2.237963
114.442265	1576.418833	5.262157	-0.021972	2.243083
115.031009	1584.485622	5.267162	-0.022086	2.248216
115.392440	1592.575338	5.272166	-0.022159	2.253332
115.621137	1600.687963	5.277171	-0.022206	2.258439
116.117225	1608.737536	5.282176	-0.022304	2.263519
116.508068	1616.807381	5.287181	-0.022381	2.268591
117.094502	1624.950029	5.292186	-0.022496	2.273713
117.116950	1633.039079	5.297190	-0.022505	2.278742
117.496683	1641.081571	5.302195	-0.022580	2.283761
117.884099	1649.122031	5.307200	-0.022657	2.288769
118.284169	1657.199902	5.312205	-0.022737	2.293790
118.603293	1665.277464	5.317210	-0.022801	2.298793
119.022766	1673.320944	5.322214	-0.022884	2.303772
119.283248	1681.416410	5.327219	-0.022938	2.308759
119.560062	1689.510993	5.332224	-0.022994	2.313737
119.823660	1697.565906	5.337229	-0.023048	2.318678
120.186364	1705.632868	5.342234	-0.023121	2.323624
120.420740	1713.694683	5.347238	-0.023170	2.328545
120.841410	1721.785192	5.352243	-0.023253	2.333489
121.550658	1729.796125	5.357248	-0.023390	2.338398
121.918238	1737.854465	5.362253	-0.023463	2.343298
122.270480	1745.949891	5.367258	-0.023534	2.348208
122.587366	1754.057166	5.372262	-0.023598	2.353111
123.004596	1762.114409	5.377267	-0.023680	2.357983
123.243618	1770.173537	5.382272	-0.023730	2.362831
123.835122	1778.196405	5.387277	-0.023845	2.367677
124.213541	1786.290445	5.392282	-0.023920	2.372537
124.504421	1794.348297	5.397286	-0.023980	2.377359
124.888726	1802.420695	5.402291	-0.024056	2.382187
125.034226	1810.500626	5.407296	-0.024088	2.386990
125.331295	1818.581154	5.412301	-0.024148	2.391797
125.824916	1826.644747	5.417306	-0.024245	2.396599
126.292287	1834.663413	5.422310	-0.024337	2.401363
126.867521	1842.705200	5.427315	-0.024449	2.406139
127.092814	1850.809624	5.432320	-0.024496	2.410915
127.701946	1858.853979	5.437325	-0.024615	2.415677
128.136380	1866.926823	5.442330	-0.024700	2.420431
128.305496	1874.992337	5.447334	-0.024737	2.425152
128.800811	1883.071869	5.452339	-0.024834	2.429897
129.219442	1891.215274	5.457344	-0.024917	2.434664
129.499060	1899.240297	5.462349	-0.024974	2.439342
129.978934	1907.259145	5.467354	-0.025068	2.444022
130.238939	1915.315009	5.472358	-0.025122	2.448699
130.612715	1923.395895	5.477363	-0.025196	2.453389
130.846564	1931.454931	5.482368	-0.025245	2.458047
131.131375	1939.511872	5.487373	-0.025303	2.462699
131.504844	1947.575654	5.492378	-0.025377	2.467353
131.988727	1955.620586	5.497382	-0.025472	2.471995
132.672654	1963.652172	5.502387	-0.025605	2.476636
132.923076	1971.721673	5.507392	-0.025656	2.481257
132.981059	1979.805576	5.512397	-0.025672	2.485864
133.330037	1987.879441	5.517402	-0.025742	2.490478
134.087043	1995.892827	5.522406	-0.025888	2.495079
134.377401	2003.981807	5.527411	-0.025947	2.499679
134.781839	2012.018630	5.532416	-0.026027	2.504251
135.116687	2020.087400	5.537421	-0.026094	2.508826
135.523067	2028.198268	5.542426	-0.026175	2.513423
135.755935	2036.234227	5.547430	-0.026223	2.517956
136.206942	2044.263245	5.552435	-0.026312	2.522493
136.389572	2052.311248	5.557440	-0.026351	2.527012
136.712395	2060.376257	5.562445	-0.026416	2.531544
137.215626	2068.432330	5.567450	-0.026515	2.536075
137.476793	2076.474245	5.572454	-0.026569	2.540572
138.007782	2084.499886	5.577459	-0.026672	2.545072
138.515308	2092.556280	5.582464	-0.026772	2.549579
138.957068	2100.629958	5.587469	-0.026859	2.554083
139.337782	2108.682114	5.592474	-0.026935	2.558563
139.629923	2116.714551	5.597478	-0.026994	2.563018
140.115821	2124.778632	5.602483	-0.027090	2.567496
140.377170	2132.855031	5.607488	-0.027143	2.571957
140.303322	2140.957957	5.612493	-0.027135	2.576402
140.543103	2149.024865	5.617498	-0.027184	2.580841
140.798050	2157.047674	5.622502	-0.027237	2.585249
141.558474	2165.068740	5.627507	-0.027383	2.589683
141.872311	2173.320899	5.632512	-0.027447	2.594205
142.164179	2181.315502	5.637517	-0.027506	2.598578
142.673702	2189.302637	5.642522	-0.027606	2.602954
142.800098	2197.320725	5.647526	-0.027634	2.607313
143.075645	2205.382219	5.652531	-0.027690	2.611698
143.184947	2213.456122	5.657536	-0.027716	2.616072
143.266488	2221.478760	5.662541	-0.027736	2.620409
143.942635	2229.453903	5.667546	-0.027867	2.624752
144.242144	2237.514760	5.672550	-0.027927	2.629110
144.455317	2245.616406	5.677555	-0.027972	2.633476
144.409334	2253.695974	5.682560	-0.027968	2.637806
144.858816	2261.692849	5.687565	-0.028057	2.642117
145.222061	2269.743752	5.692570	-0.028130	2.646445
145.373610	2277.790683	5.697574	-0.028163	2.650749
145.737160	2285.855336	5.702579	-0.028235	2.655070
146.231149	2293.875703	5.707584	-0.028332	2.659368
146.365027	2301.930337	5.712589	-0.028362	2.663654
147.097928	2309.948044	5.717594	-0.028504	2.667953
147.573070	2318.005156	5.722598	-0.028597	2.672248
148.145296	2326.075557	5.727603	-0.028709	2.676550
148.284863	2334.125278	5.732608	-0.028740	2.680806
148.900662	2342.089320	5.737613	-0.028859	2.685041
149.160300	2350.186562	5.742618	-0.028912	2.689316
149.128554	2358.270716	5.747622	-0.028912	2.693559
149.561591	2366.314010	5.752627	-0.028997	2.697804
149.925780	2374.342100	5.757632	-0.029070	2.702029
150.126133	2382.393677	5.762637	-0.029112	2.706250
150.526805	2390.454892	5.767642	-0.029192	2.710481
150.738397	2398.514390	5.772646	-0.029236	2.714693
151.301167	2406.520557	5.777651	-0.029346	2.718893
151.606616	2414.571930	5.782656	-0.029408	2.723094
151.847119	2422.615937	5.787661	-0.029457	2.727280
152.190938	2430.704216	5.792666	-0.029526	2.731489
152.329266	2438.767316	5.797670	-0.029557	2.735666
152.506405	2446.812202	5.802675	-0.029595	2.739830
153.203640	2454.810335	5.807680	-0.029730	2.743994
153.607219	2462.853275	5.812685	-0.029810	2.748158
153.868024	2470.961359	5.817690	-0.029863	2.752340
154.230860	2479.027902	5.822694	-0.029936	2.756500
154.661412	2487.043998	5.827699	-0.030021	2.760632
154.948049	2495.047092	5.832704	-0.030079	2.764743
155.237804	2503.080253	5.837709	-0.030138	2.768863
155.760438	2511.135081	5.842714	-0.030240	2.773002
156.021413	2519.153638	5.847718	-0.030294	2.777101
156.292562	2527.221721	5.852723	-0.030349	2.781219
156.848961	2535.221969	5.857728	-0.030458	2.785313
157.236204	2543.276142	5.862733	-0.030535	2.789419
157.420234	2551.380780	5.867738	-0.030574	2.793532
157.655469	2559.403156	5.872742	-0.030623	2.797601
158.244876	2567.426138	5.877747	-0.030738	2.801685
158.767983	2575.450832	5.882752	-0.030840	2.805759
158.980170	2583.486045	5.887757	-0.030884	2.809815
159.302969	2591.591778	5.892762	-0.030950	2.813907
159.344786	2599.627798	5.897766	-0.030962	2.817941
159.520465	2607.685594	5.902771	-0.031000	2.821988
160.015987	2615.709738	5.907776	-0.031097	2.826031
160.305534	2623.742284	5.912781	-0.031156	2.830061
160.556259	2631.852241	5.917786	-0.031208	2.834121
160.814249	2639.843959	5.922790	-0.031261	2.838117
161.364455	2647.843411	5.927795	-0.031368	2.842128
161.666919	2655.883194	5.932800	-0.031429	2.846138
161.805104	2663.915930	5.937805	-0.031460	2.850131
162.175020	2671.995633	5.942810	-0.031534	2.854154
162.379568	2680.012759	5.947814	-0.031577	2.858131
162.541504	2688.075063	5.952819	-0.031612	2.862122
162.959606	2696.100284	5.957824	-0.031695	2.866104
163.075180	2704.152460	5.962829	-0.031721	2.870077
163.314926	2712.244505	5.967834	-0.031771	2.874071
163.819016	2720.226796	5.972838	-0.031870	2.878019
164.125473	2728.241121	5.977843	-0.031932	2.881967
164.531473	2736.299520	5.982848	-0.032012	2.885937
164.814055	2744.319748	5.987853	-0.032070	2.889876
165.225148	2752.397560	5.992858	-0.032151	2.893844
165.671232	2760.407245	5.997862	-0.032239	2.897776
166.011376	2768.467354	6.002867	-0.032307	2.901721
166.236718	2776.498006	6.007872	-0.032354	2.905640
166.435104	2784.539387	6.012877	-0.032396	2.909557
166.795549	2792.697507	6.017882	-0.032468	2.913535
166.888739	2800.719032	6.022886	-0.032491	2.917426
167.215658	2808.717940	6.027891	-0.032556	2.921314
167.381013	2816.724041	6.032896	-0.032592	2.925192
167.596609	2824.750905	6.037901	-0.032637	2.929077
167.996793	2832.794338	6.042906	-0.032717	2.932974
168.389033	2840.817102	6.047910	-0.032795	2.936856
168.687907	2848.841999	6.052915	-0.032855	2.940729
168.776368	2856.882251	6.057920	-0.032877	2.944593
168.937134	2864.938319	6.062925	-0.032912	2.948463
169.229051	2872.997410	6.067930	-0.032971	2.952337
169.706330	2881.027640	6.072934	-0.033065	2.956201
170.053603	2889.015911	6.077939	-0.033134	2.960033
170.524475	2897.035498	6.082944	-0.033227	2.963882
170.485852	2905.100775	6.087949	-0.033225	2.967721
170.783842	2913.172599	6.092954	-0.033285	2.971575
171.148848	2921.199235	6.097958	-0.033358	2.975407
171.420790	2929.239106	6.102963	-0.033414	2.979234
171.759059	2937.273829	6.107968	-0.033481	2.983058
172.003110	2945.303320	6.112973	-0.033532	2.986870
172.521038	2953.340567	6.117978	-0.033633	2.990694
172.564096	2961.437381	6.122982	-0.033646	2.994518
172.752958	2969.448957	6.127987	-0.033686	2.998303
173.044639	2977.463225	6.132992	-0.033746	3.002091
173.235047	2985.474527	6.137997	-0.033786	3.005867
173.365002	2993.542283	6.143002	-0.033815	3.009661
173.655502	3001.568136	6.148006	-0.033874	3.013440
174.200646	3009.572863	6.153011	-0.033981	3.017216
174.387576	3017.627385	6.158016	-0.034020	3.020993
174.624910	3025.629994	6.163021	-0.034069	3.024743
175.188196	3033.672294	6.168026	-0.034179	3.028523
175.333102	3041.742321	6.173030	-0.034211	3.032291
175.823563	3049.775182	6.178035	-0.034308	3.036054
176.240561	3057.771451	6.183040	-0.034390	3.039791
176.493923	3065.805474	6.188045	-0.034442	3.043534
176.855782	3073.866615	6.193050	-0.034515	3.047289
176.891915	3081.939757	6.198054	-0.034526	3.051030
177.147435	3089.967179	6.203059	-0.034579	3.054755
177.477052	3098.003694	6.208064	-0.034645	3.058484
177.585777	3106.032883	6.213069	-0.034670	3.062194
178.048590	3114.060740	6.218074	-0.034761	3.065916
178.374582	3122.073881	6.223078	-0.034827	3.069620
178.903662	3130.188295	6.228083	-0.034930	3.073375
179.255859	3138.225455	6.233088	-0.035001	3.077082
179.404758	3146.225013	6.238093	-0.035034	3.080758
179.905138	3154.197244	6.243098	-0.035132	3.084433
180.151385	3162.235659	6.248102	-0.035183	3.088123
180.397084	3170.299596	6.253107	-0.035233	3.091819
180.755677	3178.343470	6.258112	-0.035305	3.095507
180.767200	3186.351838	6.263117	-0.035312	3.099159
181.212128	3194.396163	6.268122	-0.035400	3.102842
181.304094	3202.441658	6.273126	-0.035422	3.106505
181.651896	3210.469766	6.278131	-0.035492	3.110168
182.174044	3218.517673	6.283136	-0.035594	3.113843
182.266515	3226.549885	6.288141	-0.035616	3.117488
182.781004	3234.585516	6.293146	-0.035717	3.121148
183.027078	3242.549675	6.298150	-0.035767	3.124760
183.207516	3250.625128	6.303155	-0.035806	3.128415
183.519200	3258.672925	6.308160	-0.035869	3.132059
183.948782	3266.692987	6.313165	-0.035954	3.135691
184.184559	3274.724973	6.318170	-0.036003	3.139316
184.492952	3282.739782	6.323174	-0.036065	3.142933
184.594542	3290.812768	6.328179	-0.036089	3.146562
184.906610	3298.848084	6.333184	-0.036152	3.150179
185.093907	3306.895210	6.338189	-0.036192	3.153792
185.262009	3314.936079	6.343194	-0.036228	3.157396
185.607651	3322.941016	6.348198	-0.036297	3.160989
185.993040	3330.911497	6.353203	-0.036374	3.164564
186.296825	3338.970545	6.358208	-0.036436	3.168170
186.702803	3346.993995	6.363213	-0.036516	3.171761
187.108880	3355.041483	6.368218	-0.036597	3.175359
187.195534	3363.085453	6.373222	-0.036618	3.178937
187.584472	3371.082066	6.378227	-0.036695	3.182503
187.830942	3379.143068	6.383232	-0.036746	3.186087
187.935115	3387.185266	6.388237	-0.036770	3.189653
188.268514	3395.241483	6.393242	-0.036837	3.193231
188.537402	3403.270634	6.398246	-0.036892	3.196790
189.048751	3411.249029	6.403251	-0.036992	3.200333
189.153388	3419.297060	6.408256	-0.037017	3.203885
189.291566	3427.328209	6.413261	-0.037047	3.207428
189.801032	3435.361649	6.418266	-0.037147	3.210983
189.983300	3443.389592	6.423270	-0.037186	3.214518
190.261786	3451.453715	6.428275	-0.037243	3.218069
190.499830	3459.477961	6.433280	-0.037292	3.221597
190.636057	3467.467884	6.438285	-0.037323	3.225101
190.964987	3475.543524	6.443290	-0.037389	3.228648
191.071342	3483.594647	6.448294	-0.037413	3.232170
191.409479	3491.655937	6.453299	-0.037481	3.235703
191.640897	3499.630812	6.458304	-0.037529	3.239190
191.921562	3507.629915	6.463309	-0.037587	3.242685
192.058801	3515.686238	6.468314	-0.037617	3.246196
192.293918	3523.678355	6.473318	-0.037666	3.249679
192.282093	3531.755875	6.478323	-0.037669	3.253185
192.657891	3539.797839	6.483328	-0.037743	3.256687
193.038903	3547.753715	6.488333	-0.037819	3.260149
193.355110	3555.804292	6.493338	-0.037883	3.263645
193.418243	3563.842697	6.498342	-0.037900	3.267123
193.866647	3571.844464	6.503347	-0.037988	3.270596
194.269988	3579.917716	6.508352	-0.038068	3.274094
194.333431	3587.953806	6.513357	-0.038085	3.277559
194.525474	3595.980987	6.518362	-0.038126	3.281022
194.555825	3603.969607	6.523366	-0.038136	3.284458
194.678663	3612.034634	6.528371	-0.038164	3.287926
195.012215	3620.095839	6.533376	-0.038231	3.291398
195.496395	3628.093172	6.538381	-0.038326	3.294845
195.822692	3636.108884	6.543386	-0.038392	3.298289
195.790127	3644.153528	6.548390	-0.038391	3.301729
196.390343	3652.131111	6.553395	-0.038508	3.305160
196.648212	3660.217269	6.558400	-0.038561	3.308621
196.905879	3668.249039	6.563405	-0.038613	3.312055
197.225187	3676.319016	6.568410	-0.038678	3.315504
197.539720	3684.282720	6.573414	-0.038741	3.318905
197.756562	3692.301579	6.578419	-0.038787	3.322321
197.934301	3700.324887	6.583424	-0.038825	3.325734
197.946983	3708.357767	6.588429	-0.038832	3.329142
198.197987	3716.403073	6.593434	-0.038884	3.332560
198.410909	3724.437957	6.598438	-0.038928	3.335969
198.653246	3732.437236	6.603443	-0.038978	3.339361
198.846531	3740.502278	6.608448	-0.039019	3.342774
199.037157	3748.522600	6.613453	-0.039060	3.346166
199.525898	3756.530512	6.618458	-0.039156	3.349560
199.842882	3764.568309	6.623462	-0.039220	3.352956
199.899228	3772.645063	6.628467	-0.039235	3.356356
199.992393	3780.651061	6.633472	-0.039257	3.359724
200.236205	3788.632865	6.638477	-0.039308	3.363084
200.472102	3796.686752	6.643482	-0.039356	3.366470
200.426883	3804.743078	6.648486	-0.039353	3.369844
200.651508	3812.768778	6.653491	-0.039400	3.373211
201.132863	3820.821105	6.658496	-0.039494	3.376596
201.153206	3828.820684	6.663501	-0.039503	3.379938
201.450088	3836.838458	6.668506	-0.039563	3.383295
201.788164	3844.857113	6.673510	-0.039631	3.386650
202.147208	3852.876869	6.678515	-0.039703	3.390002
202.474558	3860.999745	6.683520	-0.039769	3.393393
202.568542	3869.018984	6.688525	-0.039791	3.396730
202.952976	3876.977461	6.693530	-0.039868	3.400048
202.987756	3884.984398	6.698534	-0.039879	3.403371
203.189840	3893.016895	6.703539	-0.039922	3.406707
203.522243	3901.005794	6.708544	-0.039989	3.410026
203.484073	3909.080195	6.713549	-0.039986	3.413364
203.765724	3917.123175	6.718554	-0.040044	3.416697
204.091600	3925.075915	6.723558	-0.040109	3.419991
204.292490	3933.116454	6.728563	-0.040152	3.423314
204.665002	3941.176581	6.733568	-0.040226	3.426647
204.753961	3949.194370	6.738573	-0.040248	3.429950
205.326667	3957.258619	6.743578	-0.040359	3.433285
205.178308	3965.284118	6.748582	-0.040336	3.436577
205.601184	3973.277610	6.753587	-0.040420	3.439872
205.842061	3981.304411	6.758592	-0.040470	3.443171
206.014558	3989.320928	6.763597	-0.040507	3.446460
206.326979	3997.386552	6.768602	-0.040570	3.449771
206.541624	4005.400724	6.773606	-0.040615	3.453055
206.723465	4013.438269	6.778611	-0.040654	3.456343
207.077023	4021.449884	6.783616	-0.040725	3.459624
207.078953	4029.474424	6.788621	-0.040730	3.462895
207.413872	4037.530597	6.793626	-0.040797	3.466187
207.577981	4045.552152	6.798630	-0.040833	3.469456
207.721112	4053.627589	6.803635	-0.040864	3.472743
207.908890	4061.649528	6.808640	-0.040904	3.476007
208.102560	4069.600878	6.813645	-0.040945	3.479239
208.520423	4077.638363	6.818650	-0.041028	3.482510
208.440864	4085.670280	6.823654	-0.041018	3.485760
208.762447	4093.674329	6.828659	-0.041083	3.489009
209.023082	4101.722446	6.833664	-0.041136	3.492270
208.985583	4109.769774	6.838669	-0.041134	3.495518
209.420812	4117.744410	6.843674	-0.041220	3.498749
209.431925	4125.776617	6.848678	-0.041227	3.501987
209.576861	4133.800471	6.853683	-0.041259	3.505223
209.872571	4141.834909	6.858688	-0.041319	3.508464
209.983656	4149.856185	6.863693	-0.041345	3.511692
210.454231	4157.919478	6.868698	-0.041437	3.514944
210.585107	4165.922318	6.873702	-0.041467	3.518159
210.768361	4173.937887	6.878707	-0.041506	3.521378
211.042114	4181.932135	6.883712	-0.041562	3.524587
211.296408	4189.943090	6.888717	-0.041614	3.527800
211.629088	4198.010217	6.893722	-0.041681	3.531035
212.011491	4206.051415	6.898726	-0.041757	3.534258
212.145489	4214.082888	6.903731	-0.041787	3.537466
212.445171	4222.105320	6.908736	-0.041848	3.540673
212.897324	4230.072735	6.913741	-0.041937	3.543860
213.276035	4238.158226	6.918746	-0.042012	3.547088
213.360762	4246.187598	6.923750	-0.042033	3.550283
213.914250	4254.282096	6.928755	-0.042141	3.553514
214.293958	4262.322366	6.933760	-0.042217	3.556716
214.544684	4270.244906	6.938765	-0.042268	3.559864
214.861907	4278.274536	6.943770	-0.042332	3.563054
214.948395	4286.298542	6.948774	-0.042353	3.566232
215.151001	4294.305408	6.953779	-0.042396	3.569403
215.565697	4302.352953	6.958784	-0.042478	3.572594
215.696842	4310.361372	6.963789	-0.042507	3.575759
215.982378	4318.375979	6.968794	-0.042565	3.578927
216.385360	4326.405924	6.973798	-0.042645	3.582102
216.720422	4334.368763	6.978803	-0.042713	3.585246
217.083518	4342.447115	6.983808	-0.042785	3.588433
217.166991	4350.505318	6.988813	-0.042806	3.591602
217.681846	4358.510972	6.993818	-0.042907	3.594759
217.969056	4366.522735	6.998822	-0.042965	3.597910
218.114985	4374.532646	7.003827	-0.042997	3.601052
218.286047	4382.562190	7.008832	-0.043034	3.604201
218.386505	4390.591893	7.013837	-0.043057	3.607345
218.673985	4398.593789	7.018842	-0.043116	3.610480
218.706768	4406.647216	7.023846	-0.043127	3.613626
219.107206	4414.681707	7.028851	-0.043206	3.616772
219.211352	4422.686566	7.033856	-0.043231	3.619895
219.416822	4430.691273	7.038861	-0.043274	3.623018
219.965362	4438.762422	7.043866	-0.043381	3.626174
220.051747	4446.774336	7.048870	-0.043402	3.629291
220.101277	4454.844798	7.053875	-0.043416	3.632428
220.280825	4462.893917	7.058880	-0.043455	3.635557
220.398987	4470.850411	7.063885	-0.043482	3.638645
220.836105	4478.880359	7.068890	-0.043568	3.641768
220.864726	4486.872933	7.073894	-0.043578	3.644863
221.084023	4494.916552	7.078899	-0.043624	3.647980
221.384914	4502.952676	7.083904	-0.043685	3.651093
221.644583	4510.988910	7.088909	-0.043738	3.654203
221.887676	4519.041338	7.093914	-0.043788	3.657316
221.964417	4527.024531	7.098918	-0.043808	3.660395
222.115883	4535.035376	7.103923	-0.043841	3.663485
222.604899	4543.080585	7.108928	-0.043937	3.666593
222.745996	4551.082350	7.113933	-0.043968	3.669673
222.676887	4559.160306	7.118938	-0.043960	3.672775
222.995433	4567.152390	7.123942	-0.044024	3.675851
223.303307	4575.147142	7.128947	-0.044086	3.678925
223.511059	4583.192066	7.133952	-0.044130	3.682013
223.653246	4591.170695	7.138957	-0.044161	3.685071
223.971561	4599.213766	7.143962	-0.044226	3.688156
224.408625	4607.244446	7.148966	-0.044312	3.691236
224.562322	4615.280229	7.153971	-0.044346	3.694309
224.826547	4623.317165	7.158976	-0.044400	3.697382
224.921751	4631.298234	7.163981	-0.044422	3.700427
225.088603	4639.329629	7.168986	-0.044458	3.703491
225.288563	4647.373808	7.173990	-0.044501	3.706558
225.485953	4655.347713	7.178995	-0.044542	3.709595
225.975880	4663.469625	7.184000	-0.044638	3.712693
226.108719	4671.517895	7.189005	-0.044668	3.715752
226.422604	4679.460794	7.194010	-0.044731	3.718773
226.590257	4687.461680	7.199014	-0.044768	3.721810
226.942440	4695.431839	7.204019	-0.044838	3.724837
227.004470	4703.523670	7.209024	-0.044855	3.727901
227.129709	4711.516582	7.214029	-0.044883	3.730926
227.439964	4719.609331	7.219034	-0.044946	3.733991
227.681732	4727.613907	7.224038	-0.044996	3.737018
227.811679	4735.571668	7.229043	-0.045025	3.740023
228.087251	4743.641129	7.234048	-0.045081	3.743070
228.238138	4751.660390	7.239053	-0.045114	3.746094
228.536502	4759.673700	7.244058	-0.045174	3.749116
228.718545	4767.724924	7.249062	-0.045213	3.752147
229.104658	4775.735199	7.254067	-0.045290	3.755165
229.431213	4783.755769	7.259072	-0.045356	3.758183
229.881911	4791.771971	7.264077	-0.045445	3.761200
230.453654	4799.755725	7.269082	-0.045556	3.764205
230.972145	4807.804422	7.274086	-0.045658	3.767230
231.370059	4815.848802	7.279091	-0.045737	3.770249
231.842611	4823.908648	7.284096	-0.045830	3.773273
232.181382	4831.904668	7.289101	-0.045898	3.776267
232.795750	4839.918185	7.294106	-0.046017	3.779272
233.119757	4847.925658	7.299110	-0.046082	3.782265
233.536916	4855.950805	7.304115	-0.046165	3.785265
233.777025	4863.983853	7.309120	-0.046214	3.788261
233.890050	4872.015825	7.314125	-0.046240	3.791251
234.227826	4880.116479	7.319130	-0.046308	3.794270
234.237714	4888.101861	7.324134	-0.046315	3.797236
234.616057	4896.056634	7.329139	-0.046390	3.800197
235.154206	4904.027765	7.334144	-0.046495	3.803165
234.992923	4912.100254	7.339149	-0.046470	3.806152
235.268196	4920.086911	7.344154	-0.046527	3.809116
235.680991	4928.153801	7.349158	-0.046608	3.812109
235.864689	4936.158546	7.354163	-0.046647	3.815072
235.958312	4944.224689	7.359168	-0.046670	3.818054
236.310246	4952.195157	7.364173	-0.046740	3.821003
236.570211	4960.183994	7.369178	-0.046794	3.823955
236.503203	4968.237651	7.374182	-0.046786	3.826921
236.718372	4976.233111	7.379187	-0.046831	3.829870
237.039223	4984.326443	7.384192	-0.046896	3.832855
237.111546	4992.325616	7.389197	-0.046914	3.835797
237.262067	5000.325709	7.394202	-0.046947	3.838739
237.694307	5008.353611	7.399206	-0.047033	3.841695
237.872265	5016.306770	7.404211	-0.047071	3.844616
238.102309	5024.401194	7.409216	-0.047118	3.847588
238.291485	5032.397659	7.414221	-0.047159	3.850520
238.467989	5040.444535	7.419226	-0.047196	3.853469
238.481714	5048.523729	7.424230	-0.047204	3.856423
238.544127	5056.479952	7.429235	-0.047220	3.859332
238.998915	5064.532745	7.434240	-0.047310	3.862281
239.061840	5072.507163	7.439245	-0.047327	3.865192
239.220525	5080.577502	7.444250	-0.047361	3.868137
239.615729	5088.588080	7.449254	-0.047440	3.871063
239.951759	5096.865498	7.454259	-0.047507	3.874083
240.195015	5104.875453	7.459264	-0.047558	3.877001
240.171192	5112.709105	7.464269	-0.047558	3.879847
240.499986	5120.718837	7.469274	-0.047624	3.882763
240.614259	5128.693669	7.474278	-0.047650	3.885659
240.728246	5136.667633	7.479283	-0.047676	3.888553
241.140103	5144.718025	7.484288	-0.047758	3.891478
241.259855	5152.766763	7.489293	-0.047785	3.894394
241.437589	5160.828907	7.494298	-0.047823	3.897315
241.678269	5168.788498	7.499302	-0.047873	3.900197
241.929158	5176.788133	7.504307	-0.047925	3.903092
242.342054	5184.833859	7.509312	-0.048006	3.906004
242.435230	5192.833046	7.514317	-0.048029	3.908891
242.954010	5200.881246	7.519322	-0.048130	3.911802
243.432905	5208.917775	7.524326	-0.048224	3.914705
243.538730	5216.911006	7.529331	-0.048249	3.917584
243.894993	5224.924331	7.534336	-0.048320	3.920472
244.304623	5232.892350	7.539341	-0.048401	3.923343
244.231855	5240.975132	7.544346	-0.048393	3.926245
244.503706	5249.003868	7.549350	-0.048448	3.929131
244.735618	5257.013633	7.554355	-0.048497	3.932007
245.027885	5265.017636	7.559360	-0.048556	3.934880
245.203184	5273.034314	7.564365	-0.048593	3.937754
245.624019	5281.056978	7.569370	-0.048677	3.940631
245.782153	5289.082940	7.574374	-0.048711	3.943504
245.829614	5297.066946	7.579379	-0.048725	3.946357
246.084727	5305.109570	7.584384	-0.048777	3.949233
246.389754	5313.150483	7.589389	-0.048839	3.952106
246.602521	5321.188729	7.594394	-0.048884	3.954976
246.740334	5329.226891	7.599398	-0.048914	3.957841
247.110511	5337.186920	7.604403	-0.048988	3.960681
247.326883	5345.212891	7.609408	-0.049033	3.963539
247.442461	5353.174009	7.614413	-0.049060	3.966371
247.657465	5361.224065	7.619418	-0.049105	3.969234
247.973383	5369.267326	7.624422	-0.049168	3.972094
248.016097	5377.312699	7.629427	-0.049181	3.974948
248.314222	5385.372132	7.634432	-0.049242	3.977810
248.507645	5393.315420	7.639437	-0.049283	3.980626
248.897517	5401.352329	7.644442	-0.049360	3.983477
248.898597	5409.399099	7.649446	-0.049365	3.986322
249.308050	5417.402687	7.654451	-0.049447	3.989157
249.427486	5425.489183	7.659456	-0.049474	3.992015
249.570305	5433.489302	7.664461	-0.049505	3.994840
249.739892	5441.536439	7.669466	-0.049542	3.997681
249.969855	5449.489141	7.674470	-0.049590	4.000487
249.932685	5457.513727	7.679475	-0.049588	4.003312
250.180019	5465.540908	7.684480	-0.049639	4.006140
250.501763	5473.528788	7.689485	-0.049703	4.008954
250.640778	5481.620360	7.694490	-0.049734	4.011800
250.782193	5489.669605	7.699494	-0.049766	4.014628
250.987456	5497.621186	7.704499	-0.049809	4.017421
251.150073	5505.653312	7.709504	-0.049844	4.020240
251.054800	5513.661476	7.714509	-0.049831	4.023045
251.067411	5521.684749	7.719514	-0.049838	4.025854
251.446160	5529.733402	7.724518	-0.049914	4.028676
251.607601	5537.734758	7.729523	-0.049949	4.031476
251.891040	5545.873244	7.734528	-0.050007	4.034324
252.216124	5553.835137	7.739533	-0.050072	4.037109
252.351847	5561.789284	7.744538	-0.050102	4.039886
252.536178	5569.807806	7.749542	-0.050141	4.042685
252.711189	5577.794717	7.754547	-0.050179	4.045471
253.141557	5585.825778	7.759552	-0.050264	4.048273
253.006012	5593.850440	7.764557	-0.050244	4.051063
253.357338	5601.874615	7.769562	-0.050314	4.053858
253.643888	5609.902682	7.774566	-0.050372	4.056652
253.968273	5617.861988	7.779571	-0.050438	4.059420
254.026129	5625.922454	7.784576	-0.050453	4.062218
254.376704	5633.891841	7.789581	-0.050524	4.064986
254.521942	5641.964423	7.794586	-0.050556	4.067785
254.509961	5649.977763	7.799590	-0.050558	4.070560
254.656703	5657.994671	7.804595	-0.050591	4.073336
254.968633	5666.061953	7.809600	-0.050654	4.076130
254.943040	5674.004712	7.814605	-0.050654	4.078874
255.209410	5682.065091	7.819610	-0.050708	4.081661
255.402577	5690.029015	7.824614	-0.050749	4.084412
255.508661	5698.090582	7.829619	-0.050774	4.087193
255.698883	5706.102733	7.834624	-0.050814	4.089957
255.757814	5714.155442	7.839629	-0.050830	4.092731
256.279723	5722.162987	7.844634	-0.050932	4.095493
256.474396	5730.176100	7.849638	-0.050973	4.098252
256.664790	5738.146699	7.854643	-0.051014	4.100993
256.853688	5746.192796	7.859648	-0.051054	4.103759
256.783919	5754.226956	7.864653	-0.051046	4.106516
256.926597	5762.237500	7.869658	-0.051077	4.109265
257.444358	5770.284900	7.874662	-0.051179	4.112030
257.538246	5778.342888	7.879667	-0.051201	4.114791
257.830638	5786.393456	7.884672	-0.051260	4.117550
258.247715	5794.337186	7.889677	-0.051343	4.120272
258.508771	5802.358804	7.894682	-0.051397	4.123018
258.828987	5810.348969	7.899686	-0.051461	4.125751
259.025448	5818.352750	7.904691	-0.051503	4.128485
259.412981	5826.436467	7.909696	-0.051580	4.131248
259.525927	5834.445899	7.914701	-0.051606	4.133980
259.783660	5842.481150	7.919706	-0.051659	4.136720
259.995860	5850.441826	7.924710	-0.051703	4.139433
260.239028	5858.469138	7.929715	-0.051753	4.142167
260.318764	5866.505799	7.934720	-0.051773	4.144900
260.497819	5874.542476	7.939725	-0.051811	4.147633
260.823435	5882.524224	7.944730	-0.051877	4.150347
260.962328	5890.628275	7.949734	-0.051908	4.153098
261.067869	5898.620107	7.954739	-0.051932	4.155809
261.533042	5906.625124	7.959744	-0.052024	4.158527
261.662113	5914.600950	7.964749	-0.052053	4.161230
261.821303	5922.624370	7.969754	-0.052087	4.163947
262.085337	5930.670800	7.974758	-0.052141	4.166671
262.436173	5938.640229	7.979763	-0.052212	4.169368
262.593171	5946.743496	7.984768	-0.052246	4.172107
262.795556	5954.731293	7.989773	-0.052288	4.174805
263.055150	5962.736348	7.994778	-0.052342	4.177508
263.292350	5970.762260	7.999782	-0.052391	4.180216
263.427290	5978.775492	8.004787	-0.052421	4.182917
263.783861	5986.775648	8.009792	-0.052492	4.185614
263.830557	5994.768823	8.014797	-0.052506	4.188304
264.067476	6002.807514	8.019802	-0.052555	4.191009
264.219986	6010.995475	8.024806	-0.052588	4.193762
264.430524	6018.936850	8.029811	-0.052632	4.196431
264.528388	6026.884122	8.034816	-0.052655	4.199098
264.509208	6034.910931	8.039821	-0.052657	4.201790
265.007976	6042.815905	8.044826	-0.052755	4.204444
265.088797	6050.909629	8.049830	-0.052775	4.207156
265.230024	6058.900389	8.054835	-0.052806	4.209831
265.655847	6066.987532	8.059840	-0.052890	4.212541
265.613326	6075.006416	8.064845	-0.052887	4.215221
265.794842	6082.975974	8.069850	-0.052926	4.217885
266.044290	6090.983234	8.074854	-0.052977	4.220560
266.271743	6098.986976	8.079859	-0.053024	4.223233
266.379311	6107.058435	8.084864	-0.053049	4.225925
266.436428	6115.030655	8.089869	-0.053065	4.228582
266.727286	6123.085527	8.094874	-0.053124	4.231267
267.104493	6131.132821	8.099878	-0.053199	4.233948
267.051729	6139.159220	8.104883	-0.053194	4.236617
267.377731	6147.128182	8.109888	-0.053260	4.239268
267.547897	6155.136774	8.114893	-0.053297	4.241930
267.681526	6163.105397	8.119898	-0.053326	4.244576
267.791364	6171.179513	8.124902	-0.053352	4.247255
267.992035	6179.170533	8.129907	-0.053394	4.249906
268.177172	6187.220789	8.134912	-0.053434	4.252575
268.460175	6195.274451	8.139917	-0.053491	4.255244
268.616309	6203.280106	8.144922	-0.053525	4.257894
268.798912	6211.275939	8.149926	-0.053564	4.260540
268.703890	6219.309768	8.154931	-0.053551	4.263194
269.015372	6227.317914	8.159936	-0.053614	4.265841
269.225937	6235.326259	8.164941	-0.053658	4.268486
269.274483	6243.396927	8.169946	-0.053672	4.271149
269.703620	6251.458032	8.174950	-0.053757	4.273809
269.971851	6259.435587	8.179955	-0.053812	4.276440
270.192715	6267.435507	8.184960	-0.053858	4.279075
270.202744	6275.462895	8.189965	-0.053865	4.281717
270.400653	6283.442078	8.194970	-0.053907	4.284342
270.725843	6291.500988	8.199974	-0.053972	4.286993
270.750112	6299.471691	8.204979	-0.053982	4.289611
271.000714	6307.523539	8.209984	-0.054033	4.292255
271.143836	6315.526911	8.214989	-0.054065	4.294881
271.381727	6323.587255	8.219994	-0.054114	4.297525
271.650803	6331.548007	8.224998	-0.054169	4.300135
271.966759	6339.572688	8.230003	-0.054233	4.302765
272.278161	6347.566250	8.235008	-0.054296	4.305383
272.439561	6355.624676	8.240013	-0.054331	4.308019
272.590508	6363.637704	8.245018	-0.054364	4.310639
272.879619	6371.667788	8.250022	-0.054423	4.313263
272.807680	6379.708271	8.255027	-0.054414	4.315887
273.009071	6387.725408	8.260032	-0.054457	4.318504
273.211791	6395.669867	8.265037	-0.054499	4.321095
273.343522	6403.679238	8.270042	-0.054529	4.323705
273.746651	6411.700944	8.275046	-0.054609	4.326320
274.010988	6419.735510	8.280051	-0.054663	4.328936
274.225939	6427.785724	8.285056	-0.054708	4.331556
274.284383	6435.760668	8.290061	-0.054724	4.334148
274.591606	6443.817807	8.295066	-0.054786	4.336767
274.790812	6451.815843	8.300070	-0.054828	4.339364
274.762727	6459.804258	8.305075	-0.054827	4.341956
274.960269	6467.828405	8.310080	-0.054869	4.344558
275.151568	6475.862399	8.315085	-0.054910	4.347163
275.310410	6483.873022	8.320090	-0.054944	4.349758
275.498292	6491.962219	8.325094	-0.054984	4.352377
275.667245	6500.025850	8.330099	-0.055021	4.354986
275.864762	6508.027163	8.335104	-0.055062	4.357573
275.937316	6515.952621	8.340109	-0.055081	4.360134
276.158479	6523.949543	8.345114	-0.055127	4.362717
276.489826	6531.978226	8.350118	-0.055193	4.365310
276.551837	6539.952041	8.355123	-0.055210	4.367881
276.965758	6547.996661	8.360128	-0.055292	4.370476
276.956789	6556.032759	8.365133	-0.055295	4.373064
277.164933	6564.089034	8.370138	-0.055339	4.375659
277.380308	6572.100539	8.375142	-0.055384	4.378237
277.596791	6580.049816	8.380147	-0.055429	4.380794
277.821576	6588.104764	8.385152	-0.055476	4.383384
277.866434	6596.084102	8.390157	-0.055489	4.385946
278.007316	6604.128738	8.395162	-0.055520	4.388529
278.267362	6612.169310	8.400166	-0.055574	4.391109
278.346738	6620.181749	8.405171	-0.055593	4.393678
278.558784	6628.261023	8.410176	-0.055638	4.396267
278.716944	6636.174377	8.415181	-0.055672	4.398802
279.076493	6644.207147	8.420186	-0.055744	4.401374
279.231531	6652.226604	8.425190	-0.055778	4.403939
279.303459	6660.241390	8.430195	-0.055796	4.406501
279.641573	6668.275234	8.435200	-0.055864	4.409069
279.791392	6676.273807	8.440205	-0.055897	4.411623
279.933486	6684.338869	8.445210	-0.055928	4.414197
280.094754	6692.412326	8.450214	-0.055963	4.416772
280.422473	6700.354780	8.455219	-0.056029	4.419304
280.539539	6708.414882	8.460224	-0.056056	4.421872
280.735492	6716.376527	8.465229	-0.056097	4.424407
280.974856	6724.412876	8.470234	-0.056147	4.426965
281.098614	6732.454645	8.475238	-0.056175	4.429522
281.321124	6740.485966	8.480243	-0.056221	4.432075
281.819813	6748.503425	8.485248	-0.056319	4.434623
281.912036	6756.483052	8.490253	-0.056341	4.437156
282.015255	6764.479933	8.495258	-0.056365	4.439693
282.140489	6772.586552	8.500262	-0.056394	4.442263
282.214500	6780.469912	8.505267	-0.056412	4.444761
282.248740	6788.533810	8.510272	-0.056423	4.447314
282.481197	6796.500172	8.515277	-0.056472	4.449836
282.673991	6804.578287	8.520282	-0.056513	4.452392
282.908328	6812.606277	8.525286	-0.056561	4.454931
282.937254	6820.646383	8.530291	-0.056571	4.457471
283.187129	6828.606358	8.535296	-0.056623	4.459985
283.255301	6836.661146	8.540301	-0.056641	4.462527
283.590428	6844.620432	8.545306	-0.056708	4.465038
283.919640	6852.705284	8.550310	-0.056774	4.467587
283.887366	6860.677981	8.555315	-0.056773	4.470099
284.098824	6868.760602	8.560320	-0.056817	4.472644
284.370892	6876.727173	8.565325	-0.056873	4.475152
284.432093	6884.745245	8.570330	-0.056889	4.477673
284.378432	6892.728323	8.575335	-0.056884	4.480182
284.527545	6900.756544	8.580339	-0.056917	4.482705
284.755511	6908.778617	8.585344	-0.056964	4.485224
285.122897	6916.794973	8.590349	-0.057038	4.487740
285.193600	6924.807877	8.595354	-0.057056	4.490253
285.263305	6932.851220	8.600359	-0.057074	4.492774
285.457897	6940.850109	8.605363	-0.057115	4.495280
285.746212	6948.882626	8.610368	-0.057173	4.497795
285.735131	6956.878486	8.615373	-0.057176	4.500297
285.875415	6964.884482	8.620378	-0.057207	4.502801
286.289306	6972.907677	8.625383	-0.057289	4.505309
286.318136	6980.907693	8.630387	-0.057300	4.507808
286.653754	6988.943710	8.635392	-0.057367	4.510318
286.889338	6996.997139	8.640397	-0.057416	4.512831
286.962088	7005.046390	8.645402	-0.057434	4.515341
286.985977	7013.058433	8.650407	-0.057444	4.517838
287.049009	7021.002454	8.655411	-0.057460	4.520312
287.279114	7029.026920	8.660416	-0.057508	4.522811
287.383438	7037.007604	8.665421	-0.057532	4.525294
287.568104	7045.005238	8.670426	-0.057572	4.527782
287.732008	7053.051696	8.675431	-0.057607	4.530283
287.678556	7061.049750	8.680435	-0.057602	4.532767
288.139756	7069.119455	8.685440	-0.057693	4.535273
288.224897	7077.116518	8.690445	-0.057714	4.537754
288.238475	7085.110351	8.695450	-0.057721	4.540233
288.630093	7093.149807	8.700455	-0.057799	4.542725
288.873126	7101.110951	8.705459	-0.057849	4.545192
288.959848	7109.180213	8.710464	-0.057870	4.547690
289.098145	7117.169928	8.715469	-0.057901	4.550162
289.338456	7125.220118	8.720474	-0.057951	4.552652
289.486046	7133.257050	8.725479	-0.057983	4.555136
289.636828	7141.249895	8.730483	-0.058016	4.557605
289.688189	7149.242495	8.735488	-0.058031	4.560073
289.932886	7157.282206	8.740493	-0.058081	4.562554
290.127861	7165.253674	8.745498	-0.058122	4.565013
290.342907	7173.359137	8.750503	-0.058167	4.567511
290.480248	7181.277798	8.755507	-0.058198	4.569951
290.606802	7189.359011	8.760512	-0.058226	4.572439
290.782851	7197.356244	8.765517	-0.058264	4.574900
291.035102	7205.393187	8.770522	-0.058316	4.577372
291.159505	7213.400369	8.775527	-0.058344	4.579833
291.314670	7221.436236	8.780531	-0.058378	4.582302
291.611984	7229.420255	8.785536	-0.058438	4.584754
291.907036	7237.459555	8.790541	-0.058498	4.587221
292.028582	7245.466966	8.795546	-0.058526	4.589677
292.461373	7253.494518	8.800551	-0.058611	4.592139
292.571648	7261.541280	8.805555	-0.058637	4.594604
292.753467	7269.618843	8.810560	-0.058675	4.597078
292.804583	7277.486693	8.815565	-0.058690	4.599486
292.961368	7285.576055	8.820570	-0.058724	4.601960
293.358777	7293.510339	8.825575	-0.058803	4.604386
293.462513	7301.561520	8.830579	-0.058827	4.606846
293.669302	7309.571011	8.835584	-0.058870	4.609292
293.881997	7317.637023	8.840589	-0.058915	4.611754
293.750422	7325.650062	8.845594	-0.058895	4.614199
293.860670	7333.704258	8.850599	-0.058921	4.616654
294.011454	7341.607055	8.855603	-0.058954	4.619063
294.333832	7349.660780	8.860608	-0.059019	4.621516
294.244981	7357.652885	8.865613	-0.059007	4.623949
294.518430	7365.703974	8.870618	-0.059063	4.626398
294.814884	7373.731747	8.875623	-0.059123	4.628839
294.797002	7381.724363	8.880627	-0.059125	4.631268
295.065982	7389.787456	8.885632	-0.059180	4.633718
295.294930	7397.798280	8.890637	-0.059227	4.636150
295.429030	7405.766899	8.895642	-0.059257	4.638568
295.620071	7413.799584	8.900647	-0.059298	4.641004
295.750351	7421.781820	8.905651	-0.059327	4.643423
295.924327	7429.802409	8.910656	-0.059364	4.645853
295.867325	7437.849297	8.915661	-0.059359	4.648290
296.049353	7445.829928	8.920666	-0.059397	4.650705
296.396946	7453.887591	8.925671	-0.059467	4.653142
296.409017	7461.885454	8.930675	-0.059474	4.655560
296.554792	7469.924145	8.935680	-0.059506	4.657989
296.849260	7477.905628	8.940685	-0.059566	4.660399
296.952376	7485.931972	8.945690	-0.059590	4.662822
297.100866	7493.898555	8.950695	-0.059623	4.665225
297.601423	7502.003429	8.955699	-0.059721	4.667669
297.937779	7510.008376	8.960704	-0.059789	4.670081
298.000827	7518.052566	8.965709	-0.059805	4.672504
298.092942	7526.085550	8.970714	-0.059827	4.674922
298.355414	7534.121549	8.975719	-0.059881	4.677340
298.427819	7541.992576	8.980723	-0.059899	4.679707
298.615250	7550.076040	8.985728	-0.059939	4.682136
298.693545	7558.015554	8.990733	-0.059959	4.684521
298.727785	7566.086801	8.995738	-0.059970	4.686945
298.959781	7574.050056	9.000743	-0.060018	4.689335
299.036596	7582.158059	9.005747	-0.060037	4.691767
299.454695	7590.139229	9.010752	-0.060120	4.694159
299.617511	7598.152090	9.015757	-0.060155	4.696560
299.829612	7606.125672	9.020762	-0.060200	4.698947
300.285037	7614.213633	9.025767	-0.060290	4.701367
300.060127	7622.133944	9.030771	-0.060253	4.703738
300.161932	7630.182815	9.035776	-0.060277	4.706144
300.562056	7638.217267	9.040781	-0.060356	4.708545
300.908481	7646.197016	9.045786	-0.060425	4.710928
301.150516	7654.316061	9.050791	-0.060475	4.713352
301.159031	7662.297220	9.055795	-0.060482	4.715733
301.442012	7670.311985	9.060800	-0.060540	4.718123
301.567838	7678.331655	9.065805	-0.060568	4.720514
301.650430	7686.330956	9.070810	-0.060588	4.722897
302.025520	7694.309738	9.075815	-0.060663	4.725272
302.074255	7702.378822	9.080819	-0.060677	4.727674
302.245126	7710.373425	9.085824	-0.060714	4.730052
302.696496	7718.422100	9.090829	-0.060803	4.732444
302.918637	7726.439140	9.095834	-0.060849	4.734826
303.103240	7734.454674	9.100839	-0.060888	4.737207
303.063147	7742.423627	9.105843	-0.060886	4.739573
303.391464	7750.457238	9.110848	-0.060952	4.741956
303.429003	7758.439278	9.115853	-0.060964	4.744323
303.578767	7766.483428	9.120858	-0.060997	4.746708
303.648511	7774.530802	9.125863	-0.061015	4.749092
303.657503	7782.495108	9.130867	-0.061021	4.751451
304.100551	7790.601277	9.135872	-0.061109	4.753849
304.142839	7798.596222	9.140877	-0.061121	4.756214
304.453798	7806.559278	9.145882	-0.061184	4.758567
304.614532	7814.545726	9.150887	-0.061219	4.760927
304.860023	7822.560498	9.155891	-0.061270	4.763294
305.005171	7830.553785	9.160896	-0.061302	4.765654
305.159683	7838.604123	9.165901	-0.061335	4.768029
305.038232	7846.613716	9.170906	-0.061318	4.770392
305.490826	7854.656953	9.175911	-0.061407	4.772762
305.558685	7862.651600	9.180915	-0.061424	4.775117
305.425374	7870.666616	9.185920	-0.061405	4.777478
305.728952	7878.657548	9.190925	-0.061466	4.779830
306.042572	7886.683454	9.195930	-0.061529	4.782190
306.184134	7894.683439	9.200935	-0.061561	4.784542
306.417092	7902.708902	9.205939	-0.061609	4.786900
306.539117	7910.759146	9.210944	-0.061637	4.789265
306.855491	7918.776908	9.215949	-0.061700	4.791618
306.782806	7926.775970	9.220954	-0.061692	4.793966
307.073000	7934.855684	9.225959	-0.061751	4.796335
307.140414	7942.797681	9.230963	-0.061768	4.798663
307.206357	7950.838380	9.235968	-0.061785	4.801019
307.289320	7958.836418	9.240973	-0.061806	4.803362
307.365319	7966.847889	9.245978	-0.061825	4.805707
307.540981	7974.880905	9.250983	-0.061863	4.808057
307.685742	7982.835217	9.255987	-0.061894	4.810383
307.787711	7990.298190	9.260992	-0.061918	4.812564
307.918642	7994.748625	9.265997	-0.061945	4.813864
308.045871	7997.240317	9.271002	-0.061970	4.814592
308.179431	7998.559054	9.276007	-0.061995	4.814976
308.225163	7999.020391	9.281011	-0.062004	4.815111
308.258966	7999.963555	9.286016	-0.062011	4.815386
308.175445	7999.965353	9.291021	-0.061995	4.815387
308.584395	7999.894072	9.296026	-0.062070	4.815364
308.572022	7999.995376	9.301031	-0.062068	4.815394
308.431662	7999.926763	9.306035	-0.062041	4.815375
308.659247	7999.920883	9.311040	-0.062084	4.815372
308.695245	8000.034744	9.316045	-0.062090	4.815405
308.799986	7999.984081	9.321050	-0.062109	4.815390
308.742427	8000.031198	9.326055	-0.062098	4.815404
308.880898	7999.999262	9.331059	-0.062124	4.815394
309.052086	7999.939010	9.336064	-0.062155	4.815375
309.060172	7999.980801	9.341069	-0.062156	4.815387
309.051399	7999.899401	9.346074	-0.062155	4.815364
309.148296	8000.016409	9.351079	-0.062172	4.815397
308.976257	7999.956889	9.356083	-0.062140	4.815381
309.130229	7999.987200	9.361088	-0.062168	4.815389
309.104144	8000.024150	9.366093	-0.062163	4.815400
309.158378	7999.995095	9.371098	-0.062173	4.815391
309.110163	8000.037023	9.376103	-0.062164	4.815404
309.204197	8000.006489	9.381107	-0.062181	4.815394
309.312879	7999.937721	9.386112	-0.062201	4.815374
309.513643	7999.975220	9.391117	-0.062238	4.815384
309.415071	7999.906228	9.396122	-0.062219	4.815364
309.492669	8000.073151	9.401127	-0.062234	4.815412
309.314035	8000.011383	9.406131	-0.062200	4.815395
309.433668	7999.920351	9.411136	-0.062222	4.815368
309.777709	7999.988011	9.416141	-0.062286	4.815386
309.561337	7999.959820	9.421146	-0.062245	4.815379
309.497783	7999.990806	9.426151	-0.062233	4.815388
309.380551	7999.946088	9.431155	-0.062211	4.815376
309.494147	8000.007795	9.436160	-0.062232	4.815393
309.627110	8000.007832	9.441165	-0.062256	4.815393
309.665210	7999.969960	9.446170	-0.062263	4.815381
309.654330	8000.033882	9.451175	-0.062261	4.815400
309.774845	7999.997374	9.456179	-0.062283	4.815389
309.787052	7999.969761	9.461184	-0.062285	4.815381
309.889945	8000.035567	9.466189	-0.062304	4.815399
309.907970	7999.924683	9.471194	-0.062307	4.815367
309.996047	8000.016964	9.476199	-0.062323	4.815394
310.083581	8000.017318	9.481203	-0.062339	4.815393
310.097913	8000.011117	9.486208	-0.062341	4.815391
310.035747	8000.012199	9.491213	-0.062329	4.815392
310.041116	7999.932100	9.496218	-0.062330	4.815369
310.155588	8000.035507	9.501223	-0.062351	4.815398
310.016339	7999.971184	9.506227	-0.062325	4.815380
310.070655	8000.008397	9.511232	-0.062335	4.815391
310.043178	8000.031430	9.516237	-0.062329	4.815398
310.084223	7999.982918	9.521242	-0.062337	4.815383
310.053763	7999.997351	9.526247	-0.062331	4.815388
310.180502	8000.016524	9.531251	-0.062354	4.815393
310.310606	8000.040029	9.536256	-0.062378	4.815399
310.355277	8000.025779	9.541261	-0.062386	4.815395
310.468203	7999.972044	9.546266	-0.062407	4.815378
310.592817	8000.052106	9.551271	-0.062430	4.815401
310.567884	8000.051667	9.556275	-0.062425	4.815401
310.517256	7999.997361	9.561280	-0.062415	4.815385
310.382992	8000.058172	9.566285	-0.062390	4.815404
310.620042	8000.065279	9.571290	-0.062433	4.815405
310.633009	8000.067605	9.576295	-0.062436	4.815405
310.697500	8000.041926	9.581299	-0.062447	4.815398
310.598820	8000.018889	9.586304	-0.062429	4.815391
310.534861	8000.000702	9.591309	-0.062416	4.815386
310.437613	7999.964863	9.596314	-0.062398	4.815376
310.709281	8000.044154	9.601319	-0.062448	4.815398
310.614148	8000.025451	9.606323	-0.062430	4.815393
310.687457	8000.003125	9.611328	-0.062444	4.815386
310.610561	8000.036028	9.616333	-0.062429	4.815396
310.679248	7999.994386	9.621338	-0.062442	4.815384
310.788326	8000.044264	9.626343	-0.062462	4.815398
310.888865	8000.004218	9.631347	-0.062480	4.815386
310.899642	8000.055675	9.636352	-0.062482	4.815401
310.987801	8000.034664	9.641357	-0.062498	4.815394
310.962011	7999.964736	9.646362	-0.062493	4.815374
310.940038	8000.084056	9.651367	-0.062488	4.815409
310.905618	8000.017191	9.656371	-0.062482	4.815390
310.829534	8000.042626	9.661376	-0.062467	4.815397
311.110857	8000.057948	9.666381	-0.062519	4.815400
310.930794	8000.030356	9.671386	-0.062485	4.815393
310.968958	8000.079060	9.676391	-0.062492	4.815407
310.748978	8000.041187	9.681395	-0.062451	4.815397
311.037748	8000.017085	9.686400	-0.062504	4.815389
311.090511	8000.101303	9.691405	-0.062514	4.815413
311.041406	8000.068398	9.696410	-0.062505	4.815404
311.174893	8000.098373	9.701415	-0.062529	4.815412
310.929940	8000.017333	9.706419	-0.062483	4.815390
310.875704	8000.013202	9.711424	-0.062473	4.815389
311.022282	8000.030567	9.716429	-0.062500	4.815393
311.131409	8000.014178	9.721434	-0.062520	4.815388
311.188719	8000.011895	9.726439	-0.062530	4.815387
311.097149	8000.045624	9.731443	-0.062513	4.815397
311.185765	8000.066305	9.736448	-0.062529	4.815403
311.384253	8000.102702	9.741453	-0.062566	4.815412
311.148211	8000.050667	9.746458	-0.062522	4.815398
311.307079	8000.112059	9.751463	-0.062551	4.815415
311.298190	8000.063788	9.756467	-0.062549	4.815401
311.298802	8000.070185	9.761472	-0.062549	4.815403
311.154513	8000.091283	9.766477	-0.062522	4.815410
311.167356	8000.054060	9.771482	-0.062524	4.815399
311.200752	8000.087721	9.776487	-0.062530	4.815409
311.292155	8000.090278	9.781491	-0.062546	4.815409
311.220715	8000.046314	9.786496	-0.062533	4.815397
311.340389	8000.010861	9.791501	-0.062555	4.815386
311.350073	8000.022753	9.796506	-0.062556	4.815389
311.257500	8000.096013	9.801511	-0.062539	4.815411
311.308149	8000.050865	9.806515	-0.062548	4.815398
311.199779	8000.026598	9.811520	-0.062527	4.815391
311.332364	8000.104656	9.816525	-0.062552	4.815413
311.317700	8000.059495	9.821530	-0.062549	4.815400
311.669683	8000.118744	9.826535	-0.062614	4.815416
311.477670	8000.039647	9.831539	-0.062578	4.815394
311.452588	8000.029586	9.836544	-0.062573	4.815391
311.441169	8000.060368	9.841549	-0.062570	4.815400
311.321504	7999.992090	9.846554	-0.062548	4.815380
311.304187	7999.993915	9.851559	-0.062544	4.815381
311.590966	8000.089492	9.856563	-0.062598	4.815408
311.438979	8000.049538	9.861568	-0.062569	4.815397
311.399701	8000.068101	9.866573	-0.062561	4.815402
311.292375	8000.037437	9.871578	-0.062541	4.815394
311.195368	8000.075352	9.876583	-0.062523	4.815405
311.138553	8000.059420	9.881587	-0.062512	4.815401
311.476760	8000.087443	9.886592	-0.062574	4.815408
311.322849	8000.132966	9.891597	-0.062546	4.815422
311.219592	8000.010449	9.896602	-0.062526	4.815386
311.569599	8000.125244	9.901607	-0.062591	4.815418
311.544374	8000.066013	9.906611	-0.062586	4.815401
311.404785	8000.083982	9.911616	-0.062560	4.815407
311.375406	8000.118742	9.916621	-0.062554	4.815417
311.431612	7999.997797	9.921626	-0.062564	4.815382
311.697845	8000.042799	9.926631	-0.062613	4.815394
311.309536	8000.006411	9.931635	-0.062541	4.815385
311.427462	8000.028647	9.936640	-0.062562	4.815391
311.395950	8000.081541	9.941645	-0.062556	4.815406
311.272435	8000.050610	9.946650	-0.062533	4.815398
311.499276	8000.055411	9.951655	-0.062575	4.815398
311.494769	8000.027520	9.956659	-0.062574	4.815390
311.381070	8000.096154	9.961664	-0.062552	4.815411
311.478899	8000.126608	9.966669	-0.062570	4.815419
311.592386	8000.047229	9.971674	-0.062591	4.815395
311.759686	8000.147241	9.976679	-0.062622	4.815424
311.629546	8000.100167	9.981683	-0.062597	4.815411
311.579603	8000.037319	9.986688	-0.062588	4.815393
311.671777	8000.081575	9.991693	-0.062605	4.815405
311.432850	8000.060488	9.996698	-0.062560	4.815400
311.673339	8000.117889	10.001703	-0.062604	4.815416
311.607442	8000.084706	10.006707	-0.062592	4.815406
311.720551	8000.038455	10.011712	-0.062613	4.815392
311.682408	8000.084826	10.016717	-0.062605	4.815406
311.472286	8000.015050	10.021722	-0.062566	4.815387
311.602441	8000.031075	10.026727	-0.062590	4.815391
311.454855	8000.036086	10.031731	-0.062562	4.815393
311.701486	8000.052972	10.036736	-0.062607	4.815397
312.046437	8000.137758	10.041741	-0.062671	4.815420
311.889700	8000.040006	10.046746	-0.062642	4.815392
311.845438	8000.112998	10.051751	-0.062633	4.815414
311.916700	8000.114152	10.056755	-0.062646	4.815414
311.841933	8000.062651	10.061760	-0.062632	4.815399
311.766343	8000.134055	10.066765	-0.062618	4.815420
311.728293	8000.056440	10.071770	-0.062610	4.815398
311.780068	8000.078649	10.076775	-0.062620	4.815404
311.684022	8000.051379	10.081779	-0.062602	4.815396
311.691251	8000.016200	10.086784	-0.062603	4.815386
311.841492	8000.094552	10.091789	-0.062630	4.815408
311.900876	8000.023896	10.096794	-0.062641	4.815387
311.800537	8000.115199	10.101799	-0.062622	4.815414
311.773014	8000.083719	10.106803	-0.062617	4.815405
311.850496	8000.081771	10.111808	-0.062631	4.815404
311.790650	8000.108543	10.116813	-0.062619	4.815413
311.956527	8000.068511	10.121818	-0.062650	4.815400
312.053728	8000.076509	10.126823	-0.062668	4.815402
312.023450	8000.046053	10.131827	-0.062662	4.815393
311.934036	8000.017823	10.136832	-0.062645	4.815385
312.009122	8000.056452	10.141837	-0.062659	4.815396
311.970792	8000.021587	10.146842	-0.062651	4.815386
311.906043	8000.079275	10.151847	-0.062639	4.815404
311.828537	8000.076896	10.156851	-0.062624	4.815403
311.918223	7999.986434	10.161856	-0.062640	4.815376
312.018436	8000.069302	10.166861	-0.062659	4.815400
311.892529	8000.025503	10.171866	-0.062635	4.815388
312.047744	8000.082561	10.176871	-0.062664	4.815404
312.054214	8000.084780	10.181875	-0.062665	4.815404
312.119989	8000.104015	10.186880	-0.062677	4.815410
312.165888	8000.105818	10.191885	-0.062685	4.815410
312.011655	8000.041242	10.196890	-0.062656	4.815392
311.985443	8000.107051	10.201895	-0.062651	4.815411
311.966696	8000.090681	10.206899	-0.062647	4.815407
311.866181	8000.022720	10.211904	-0.062628	4.815387
312.141853	8000.110634	10.216909	-0.062679	4.815412
312.140116	8000.069961	10.221914	-0.062678	4.815400
312.344936	8000.078674	10.226919	-0.062716	4.815401
312.166647	8000.068211	10.231923	-0.062683	4.815399
312.044307	8000.030885	10.236928	-0.062660	4.815389
312.185720	8000.139020	10.241933	-0.062686	4.815420
312.076321	8000.071980	10.246938	-0.062665	4.815401
311.979044	8000.134474	10.251943	-0.062647	4.815419
311.976580	8000.106616	10.256947	-0.062646	4.815411
312.031854	8000.087198	10.261952	-0.062656	4.815405
311.848113	8000.055268	10.266957	-0.062621	4.815397
311.947648	7999.979933	10.271962	-0.062639	4.815375
312.156712	7999.996197	10.276967	-0.062678	4.815378
312.017004	8000.048368	10.281971	-0.062652	4.815394
312.033035	8000.073191	10.286976	-0.062655	4.815401
312.110289	8000.061619	10.291981	-0.062669	4.815398
311.906390	8000.062490	10.296986	-0.062630	4.815399
312.063054	8000.080024	10.301991	-0.062659	4.815403
312.117463	8000.030662	10.306995	-0.062669	4.815389
312.104809	8000.040046	10.312000	-0.062666	4.815391
312.262303	8000.067214	10.317005	-0.062695	4.815399
311.996154	8000.046744	10.322010	-0.062646	4.815394
312.265658	8000.100352	10.327015	-0.062696	4.815408
312.157547	8000.077157	10.332019	-0.062675	4.815402
312.201160	8000.081060	10.337024	-0.062683	4.815403
312.290527	8000.103893	10.342029	-0.062699	4.815409
312.264726	8000.037169	10.347034	-0.062694	4.815390
312.302691	8000.067700	10.352039	-0.062701	4.815399
311.946137	8000.083143	10.357043	-0.062634	4.815405
312.072831	8000.002913	10.362048	-0.062658	4.815381
312.256062	8000.064711	10.367053	-0.062691	4.815398
312.042081	7999.997007	10.372058	-0.062651	4.815379
312.151516	8000.094992	10.377063	-0.062671	4.815407
312.168131	8000.080277	10.382067	-0.062674	4.815403
312.128254	8000.007976	10.387072	-0.062666	4.815382
312.341016	8000.098055	10.392077	-0.062706	4.815407
312.324975	8000.042181	10.397082	-0.062702	4.815391
312.391694	8000.038985	10.402087	-0.062715	4.815390
312.410023	8000.065985	10.407091	-0.062718	4.815398
312.632541	8000.063233	10.412096	-0.062759	4.815396
312.560559	8000.151800	10.417101	-0.062745	4.815422
312.067721	8000.062371	10.422106	-0.062653	4.815398
312.255570	8000.084698	10.427111	-0.062688	4.815404
312.248855	8000.043943	10.432115	-0.062686	4.815392
312.303111	8000.015957	10.437120	-0.062696	4.815384
312.427294	8000.099223	10.442125	-0.062719	4.815407
312.452839	8000.010904	10.447130	-0.062723	4.815381
312.362608	8000.043586	10.452135	-0.062706	4.815391
312.174282	8000.048990	10.457139	-0.062671	4.815394
312.187671	8000.080183	10.462144	-0.062673	4.815403
312.346883	8000.110586	10.467149	-0.062702	4.815411
312.287120	8000.039024	10.472154	-0.062691	4.815390
312.590508	8000.052577	10.477159	-0.062747	4.815393
312.540763	8000.052795	10.482163	-0.062738	4.815393
312.424451	8000.014499	10.487168	-0.062716	4.815383
312.586403	8000.145423	10.492173	-0.062746	4.815420
312.621143	8000.064737	10.497178	-0.062752	4.815396
312.552034	8000.043257	10.502183	-0.062739	4.815390
312.383300	8000.094947	10.507187	-0.062707	4.815406
312.492038	8000.032591	10.512192	-0.062727	4.815388
312.570361	8000.081962	10.517197	-0.062741	4.815402
312.209548	8000.124055	10.522202	-0.062674	4.815416
312.260855	8000.130224	10.527207	-0.062683	4.815417
312.325938	8000.100279	10.532211	-0.062695	4.815408
312.178692	8000.090330	10.537216	-0.062667	4.815406
312.225643	8000.113529	10.542221	-0.062675	4.815413
312.248853	8000.018758	10.547226	-0.062679	4.815385
312.478781	8000.092019	10.552231	-0.062722	4.815405
312.447613	8000.098958	10.557235	-0.062716	4.815407
312.332836	8000.086341	10.562240	-0.062694	4.815404
312.612524	8000.142257	10.567245	-0.062746	4.815419
312.619049	8000.091032	10.572250	-0.062747	4.815404
312.516540	8000.128856	10.577255	-0.062728	4.815416
312.499029	8000.081509	10.582259	-0.062724	4.815402
312.403866	8000.033944	10.587264	-0.062706	4.815389
312.427808	8000.073863	10.592269	-0.062710	4.815400
312.204547	8000.082963	10.597274	-0.062668	4.815404
312.475668	8000.123772	10.602279	-0.062718	4.815414
312.263783	8000.100994	10.607283	-0.062679	4.815409
312.275952	8000.054139	10.612288	-0.062681	4.815395
312.437698	8000.071758	10.617293	-0.062711	4.815399
312.235693	8000.085486	10.622298	-0.062673	4.815404
312.279609	8000.085119	10.627303	-0.062680	4.815404
312.512154	8000.107118	10.632307	-0.062724	4.815409
312.584078	7999.993914	10.637312	-0.062737	4.815376
312.456610	8000.021704	10.642317	-0.062713	4.815385
312.438358	7999.991447	10.647322	-0.062709	4.815376
312.457529	8000.062284	10.652327	-0.062712	4.815397
312.435410	8000.036238	10.657331	-0.062708	4.815389
312.395485	7999.992796	10.662336	-0.062700	4.815377
312.600033	8000.012192	10.667341	-0.062738	4.815381
312.640270	8000.000006	10.672346	-0.062745	4.815378
312.737493	8000.091377	10.677351	-0.062763	4.815404
312.590183	8000.062188	10.682355	-0.062735	4.815396
312.479643	8000.044296	10.687360	-0.062714	4.815391
312.541571	8000.092327	10.692365	-0.062725	4.815405
312.653906	8000.027892	10.697370	-0.062746	4.815386
312.866106	8000.053830	10.702375	-0.062785	4.815392
312.712154	8000.028805	10.707379	-0.062756	4.815386
312.703194	8000.038251	10.712384	-0.062754	4.815389
312.768187	8000.018993	10.717389	-0.062766	4.815383
312.802462	8000.055877	10.722394	-0.062772	4.815393
312.648491	8000.051161	10.727399	-0.062743	4.815393
312.604334	8000.109191	10.732403	-0.062735	4.815410
312.786794	8000.114327	10.737408	-0.062768	4.815410
312.753770	8000.127649	10.742413	-0.062762	4.815414
312.648199	8000.074567	10.747418	-0.062742	4.815399
312.648501	8000.020033	10.752423	-0.062742	4.815384
312.469568	8000.088656	10.757427	-0.062708	4.815404
312.569104	8000.043249	10.762432	-0.062726	4.815391
312.593848	8000.086388	10.767437	-0.062731	4.815403
312.620204	8000.065421	10.772442	-0.062735	4.815397
312.604369	8000.033066	10.777447	-0.062732	4.815388
312.553917	8000.078165	10.782451	-0.062722	4.815401
312.764759	8000.080565	10.787456	-0.062761	4.815401
312.781411	8000.092572	10.792461	-0.062764	4.815404
312.672345	8000.012711	10.797466	-0.062744	4.815381
312.867432	8000.062948	10.802471	-0.062780	4.815395
312.900911	8000.050651	10.807475	-0.062786	4.815391
312.730974	8000.026430	10.812480	-0.062754	4.815385
312.868466	8000.117400	10.817485	-0.062779	4.815411
312.746982	8000.059778	10.822490	-0.062756	4.815395
312.738767	8000.110922	10.827495	-0.062754	4.815410
312.723815	8000.095684	10.832499	-0.062751	4.815405
312.856448	8000.055101	10.837504	-0.062776	4.815393
312.937047	8000.068169	10.842509	-0.062790	4.815396
312.708075	7999.994870	10.847514	-0.062747	4.815376
312.694320	8000.041647	10.852519	-0.062744	4.815390
312.708600	8000.012997	10.857523	-0.062747	4.815381
312.729134	7999.986590	10.862528	-0.062750	4.815374
313.031755	8000.099537	10.867533	-0.062806	4.815405
312.756455	8000.006230	10.872538	-0.062755	4.815379
312.706459	8000.003238	10.877543	-0.062745	4.815379
312.575017	8000.073716	10.882547	-0.062720	4.815400
312.844537	7999.980889	10.887552	-0.062770	4.815371
313.031487	8000.087644	10.892557	-0.062805	4.815402
312.846346	8000.021484	10.897562	-0.062770	4.815383
312.986210	8000.063325	10.902567	-0.062796	4.815395
312.828646	8000.104511	10.907571	-0.062766	4.815408
312.704131	7999.999809	10.912576	-0.062743	4.815378
312.730814	8000.020534	10.917581	-0.062747	4.815384
312.724417	8000.023608	10.922586	-0.062746	4.815385
312.483001	8000.024926	10.927591	-0.062701	4.815386
312.608501	8000.016291	10.932595	-0.062724	4.815383
312.674127	7999.995975	10.937600	-0.062736	4.815377
312.745243	8000.038813	10.942605	-0.062749	4.815389
312.659050	8000.018119	10.947610	-0.062732	4.815383
312.796029	8000.046016	10.952615	-0.062758	4.815391
312.871168	8000.054717	10.957619	-0.062771	4.815393
312.881870	8000.052731	10.962624	-0.062773	4.815392
312.918361	8000.085376	10.967629	-0.062779	4.815402
312.804295	7999.996880	10.972634	-0.062758	4.815376
312.771765	8000.011279	10.977639	-0.062752	4.815381
312.740526	8000.075936	10.982643	-0.062745	4.815400
312.725335	8000.009388	10.987648	-0.062742	4.815380
312.686911	8000.128439	10.992653	-0.062735	4.815415
312.643337	8000.019735	10.997658	-0.062726	4.815384
312.879185	8000.003308	11.002663	-0.062770	4.815378
312.908959	8000.076460	11.007667	-0.062775	4.815399
312.796633	7999.969822	11.012672	-0.062754	4.815369
312.860717	8000.053161	11.017677	-0.062766	4.815393
312.888619	7999.979845	11.022682	-0.062771	4.815371
312.835727	7999.988562	11.027687	-0.062760	4.815374
312.754201	8000.026733	11.032691	-0.062745	4.815385
312.896172	8000.013027	11.037696	-0.062771	4.815381
312.979297	8000.007965	11.042701	-0.062786	4.815379
312.848495	7999.955534	11.047706	-0.062762	4.815364
312.920614	8000.115966	11.052711	-0.062775	4.815411
312.773458	8000.125258	11.057715	-0.062747	4.815414
313.021302	8000.065207	11.062720	-0.062793	4.815395
312.813721	8000.115185	11.067725	-0.062754	4.815411
312.730810	8000.092407	11.072730	-0.062738	4.815405
312.930717	8000.097832	11.077735	-0.062775	4.815405
312.773913	8000.079173	11.082739	-0.062746	4.815401
312.990122	7999.985463	11.087744	-0.062786	4.815372
313.012246	8000.036041	11.092749	-0.062790	4.815387
312.741852	7999.970607	11.097754	-0.062739	4.815369
312.869909	7999.980185	11.102759	-0.062762	4.815371
312.901954	8000.077958	11.107763	-0.062768	4.815400
312.876827	8000.028347	11.112768	-0.062763	4.815385
312.916708	8000.087770	11.117773	-0.062770	4.815403
312.976155	7999.946569	11.122778	-0.062781	4.815361
312.968430	7999.977412	11.127783	-0.062779	4.815370
312.820974	8000.072210	11.132787	-0.062752	4.815399
312.651907	8000.069381	11.137792	-0.062720	4.815399
312.888089	8000.137403	11.142797	-0.062764	4.815417
313.033948	8000.015804	11.147802	-0.062790	4.815381
313.091677	8000.006046	11.152807	-0.062801	4.815378
313.116959	8000.082329	11.157811	-0.062805	4.815400
313.101177	8000.064939	11.162816	-0.062802	4.815395
312.921132	8000.106822	11.167821	-0.062768	4.815408
312.890960	8000.016510	11.172826	-0.062762	4.815382
313.100930	7999.991104	11.177831	-0.062801	4.815374
312.914763	8000.045712	11.182835	-0.062766	4.815390
313.031147	8000.021961	11.187840	-0.062787	4.815383
313.187197	8000.087586	11.192845	-0.062816	4.815401
313.051028	8000.048961	11.197850	-0.062791	4.815391
312.970427	8000.055081	11.202855	-0.062775	4.815393
312.986810	8000.001882	11.207859	-0.062778	4.815377
313.021093	7999.984253	11.212864	-0.062784	4.815372
312.942420	8000.023540	11.217869	-0.062769	4.815384
313.060372	8000.083189	11.222874	-0.062791	4.815401
313.337009	8000.067440	11.227879	-0.062842	4.815395
313.294105	8000.029291	11.232883	-0.062834	4.815384
312.985895	8000.019881	11.237888	-0.062776	4.815383
313.382933	8000.103396	11.242893	-0.062850	4.815405
313.247168	8000.054088	11.247898	-0.062824	4.815391
313.169520	8000.092324	11.252903	-0.062809	4.815403
313.137858	8000.120633	11.257907	-0.062803	4.815411
313.173848	8000.057070	11.262912	-0.062810	4.815393
313.051571	8000.091359	11.267917	-0.062787	4.815403
313.031118	8000.031136	11.272922	-0.062782	4.815386
313.197601	8000.049903	11.277927	-0.062813	4.815390
313.287960	8000.073821	11.282931	-0.062830	4.815397
313.180279	7999.995050	11.287936	-0.062809	4.815375
313.111418	8000.097564	11.292941	-0.062796	4.815405
313.041247	8000.013002	11.297946	-0.062783	4.815380
313.102045	8000.002226	11.302951	-0.062794	4.815377
313.376227	8000.051638	11.307955	-0.062845	4.815390
313.220456	7999.954968	11.312960	-0.062815	4.815363
313.352805	8000.047991	11.317965	-0.062840	4.815389
313.062644	7999.964058	11.322970	-0.062785	4.815366
313.072703	7999.996265	11.327975	-0.062787	4.815375
313.139859	8000.107447	11.332979	-0.062799	4.815408
313.084006	7999.951507	11.337984	-0.062788	4.815362
313.421259	7999.997688	11.342989	-0.062851	4.815374
313.240122	8000.022450	11.347994	-0.062817	4.815382
313.228123	8000.016881	11.352999	-0.062814	4.815381
313.218119	7999.995311	11.358003	-0.062812	4.815375
313.467010	7999.942760	11.363008	-0.062858	4.815358
313.422493	8000.051022	11.368013	-0.062850	4.815390
313.286302	8000.026292	11.373018	-0.062824	4.815383
313.477938	8000.029442	11.378023	-0.062860	4.815383
313.533156	8000.085914	11.383027	-0.062870	4.815399
313.349916	8000.008028	11.388032	-0.062835	4.815378
313.347898	8000.092410	11.393037	-0.062834	4.815402
313.176124	8000.046781	11.398042	-0.062802	4.815390
313.267696	8000.053617	11.403047	-0.062819	4.815391
313.402612	8000.101790	11.408051	-0.062844	4.815405
313.332763	8000.007613	11.413056	-0.062830	4.815378
313.526087	8000.067442	11.418061	-0.062866	4.815394
313.131064	8000.048041	11.423066	-0.062792	4.815390
313.283513	8000.041991	11.428071	-0.062820	4.815388
313.272854	8000.042857	11.433075	-0.062818	4.815388
313.216021	8000.009822	11.438080	-0.062807	4.815379
313.465133	8000.021408	11.443085	-0.062853	4.815381
313.502829	7999.986733	11.448090	-0.062860	4.815371
313.358637	8000.017452	11.453095	-0.062833	4.815380
313.523316	8000.087496	11.458099	-0.062863	4.815400
313.460918	8000.035129	11.463104	-0.062851	4.815385
313.502065	8000.122365	11.468109	-0.062859	4.815410
313.376948	8000.032615	11.473114	-0.062835	4.815385
313.426717	8000.074032	11.478119	-0.062844	4.815397
313.330839	8000.088450	11.483123	-0.062826	4.815401
313.285117	7999.979708	11.488128	-0.062817	4.815370
313.453783	8000.071196	11.493133	-0.062848	4.815396
313.397054	8000.038162	11.498138	-0.062837	4.815386
313.289167	8000.100481	11.503143	-0.062817	4.815405
313.283567	8000.092880	11.508147	-0.062816	4.815403
313.403136	8000.027496	11.513152	-0.062838	4.815383
313.585143	8000.034762	11.518157	-0.062871	4.815385
313.489179	8000.043834	11.523162	-0.062853	4.815388
313.536299	8000.056347	11.528167	-0.062862	4.815391
313.429976	8000.075936	11.533171	-0.062841	4.815397
313.300020	8000.021380	11.538176	-0.062817	4.815382
313.514998	8000.122187	11.543181	-0.062857	4.815410
313.535527	8000.051954	11.548186	-0.062860	4.815390
313.414213	8000.058468	11.553191	-0.062837	4.815392
313.655439	8000.114817	11.558195	-0.062882	4.815408
313.585021	8000.100796	11.563200	-0.062869	4.815404
313.692622	8000.138897	11.568205	-0.062888	4.815414
313.455805	8000.076155	11.573210	-0.062844	4.815397
313.495529	8000.015861	11.578215	-0.062851	4.815380
313.686421	8000.059617	11.583219	-0.062886	4.815391
313.537465	8000.044295	11.588224	-0.062858	4.815388
313.490998	8000.118321	11.593229	-0.062849	4.815409
313.603654	8000.029306	11.598234	-0.062870	4.815383
313.721045	8000.017331	11.603239	-0.062892	4.815379
313.612533	8000.123464	11.608243	-0.062871	4.815410
313.527018	8000.111331	11.613248	-0.062855	4.815407
313.470286	8000.071884	11.618253	-0.062844	4.815396
313.456655	8000.001085	11.623258	-0.062841	4.815375
313.608659	8000.039921	11.628263	-0.062869	4.815386
313.861188	8000.093251	11.633267	-0.062916	4.815400
313.604907	8000.045151	11.638272	-0.062868	4.815388
313.646851	8000.114230	11.643277	-0.062875	4.815408
313.687885	8000.076403	11.648282	-0.062883	4.815396
313.801425	8000.026953	11.653287	-0.062904	4.815381
313.675919	8000.093255	11.658291	-0.062880	4.815401
313.627536	8000.056084	11.663296	-0.062871	4.815391
313.670752	8000.120908	11.668301	-0.062878	4.815409
313.700256	8000.091442	11.673306	-0.062884	4.815401
313.644680	8000.080875	11.678311	-0.062873	4.815398
313.644777	8000.055197	11.683315	-0.062873	4.815390
313.652066	7999.958022	11.688320	-0.062874	4.815362
313.642813	8000.073283	11.693325	-0.062872	4.815396
313.697466	8000.059198	11.698330	-0.062882	4.815391
314.018017	8000.019593	11.703335	-0.062941	4.815378
313.850652	8000.076650	11.708339	-0.062910	4.815396
313.760927	8000.032381	11.713344	-0.062893	4.815383
313.759073	8000.092182	11.718349	-0.062892	4.815401
313.608964	8000.016982	11.723354	-0.062864	4.815380
313.736171	7999.969896	11.728359	-0.062887	4.815365
313.905323	8000.042152	11.733363	-0.062918	4.815385
313.506988	8000.025902	11.738368	-0.062844	4.815383
313.498073	8000.082380	11.743373	-0.062842	4.815399
313.556165	8000.088661	11.748378	-0.062852	4.815401
313.633763	8000.023650	11.753383	-0.062866	4.815381
313.788293	8000.059321	11.758387	-0.062895	4.815391
313.700645	7999.983019	11.763392	-0.062878	4.815369
313.747244	8000.076760	11.768397	-0.062887	4.815396
313.787294	8000.065640	11.773402	-0.062894	4.815393
313.658057	8000.045300	11.778407	-0.062870	4.815388
313.814915	8000.112008	11.783411	-0.062898	4.815406
313.992648	8000.008039	11.788416	-0.062931	4.815375
313.820073	8000.056458	11.793421	-0.062899	4.815390
313.650729	8000.050418	11.798426	-0.062867	4.815389
313.681864	8000.026323	11.803431	-0.062872	4.815382
313.825658	8000.083195	11.808435	-0.062899	4.815398
313.751156	7999.985733	11.813440	-0.062885	4.815370
313.827336	8000.078895	11.818445	-0.062899	4.815397
313.720212	8000.050370	11.823450	-0.062878	4.815389
313.827659	8000.035023	11.828455	-0.062898	4.815384
313.863982	8000.055908	11.833459	-0.062905	4.815390
313.748733	8000.043282	11.838464	-0.062883	4.815387
313.819752	8000.136359	11.843469	-0.062896	4.815414
313.719761	8000.053438	11.848474	-0.062877	4.815390
313.660282	7999.990431	11.853479	-0.062866	4.815372
313.810700	8000.115821	11.858483	-0.062893	4.815408
313.764806	8000.086174	11.863488	-0.062884	4.815399
313.857886	8000.088760	11.868493	-0.062901	4.815399
313.721612	8000.072578	11.873498	-0.062876	4.815395
313.649263	8000.048906	11.878503	-0.062862	4.815389
313.785246	8000.069306	11.883507	-0.062887	4.815394
313.764538	8000.066798	11.888512	-0.062883	4.815394
313.849052	8000.091689	11.893517	-0.062898	4.815400
313.890333	8000.110519	11.898522	-0.062906	4.815406
313.722444	8000.077780	11.903527	-0.062874	4.815397
313.696011	8000.071971	11.908531	-0.062869	4.815395
313.675269	8000.049154	11.913536	-0.062865	4.815389
313.889640	8000.106127	11.918541	-0.062904	4.815404
313.943646	8000.082412	11.923546	-0.062914	4.815397
313.972963	8000.083940	11.928551	-0.062919	4.815398
313.882280	8000.141200	11.933555	-0.062902	4.815415
314.015826	8000.124148	11.938560	-0.062927	4.815409
313.823900	8000.080321	11.943565	-0.062891	4.815397
313.862501	8000.056351	11.948570	-0.062898	4.815390
313.901133	8000.046276	11.953575	-0.062905	4.815387
313.988356	8000.075487	11.958579	-0.062920	4.815395
313.686957	8000.051224	11.963584	-0.062864	4.815390
313.891531	8000.115517	11.968589	-0.062902	4.815407
313.866725	8000.078737	11.973594	-0.062897	4.815397
313.874576	8000.068152	11.978599	-0.062898	4.815394
313.772605	8000.131638	11.983603	-0.062879	4.815413
313.769838	8000.040709	11.988608	-0.062878	4.815386
313.903576	8000.096345	11.993613	-0.062903	4.815402
313.886184	8000.089617	11.998618	-0.062899	4.815400
313.937405	8000.060511	12.003623	-0.062908	4.815391
313.916050	8000.115714	12.008627	-0.062904	4.815407
313.750915	8000.022094	12.013632	-0.062873	4.815381
313.970230	8000.051357	12.018637	-0.062914	4.815388
313.867264	8000.062450	12.023642	-0.062894	4.815392
313.818739	8000.095824	12.028647	-0.062885	4.815402
313.971799	8000.154988	12.033651	-0.062913	4.815419
313.908529	8000.082296	12.038656	-0.062901	4.815398
313.974888	8000.076957	12.043661	-0.062913	4.815396
313.967005	8000.085351	12.048666	-0.062911	4.815398
314.133298	8000.068842	12.053671	-0.062942	4.815393
314.061922	8000.096493	12.058675	-0.062928	4.815401
313.760908	8000.021998	12.063680	-0.062872	4.815381
314.012819	8000.117004	12.068685	-0.062919	4.815407
313.954470	8000.097839	12.073690	-0.062907	4.815402
314.028217	8000.115070	12.078695	-0.062921	4.815407
313.858955	8000.152855	12.083699	-0.062889	4.815419
314.028125	8000.107533	12.088704	-0.062920	4.815404
314.036638	8000.094822	12.093709	-0.062922	4.815401
313.855434	8000.093929	12.098714	-0.062888	4.815401
313.902467	7999.996344	12.103719	-0.062896	4.815373
313.997793	8000.090892	12.108723	-0.062913	4.815400
313.907266	8000.073332	12.113728	-0.062896	4.815395
313.901869	8000.067872	12.118733	-0.062895	4.815394
313.865203	8000.058686	12.123738	-0.062888	4.815391
313.920927	8000.083100	12.128743	-0.062898	4.815398
313.828208	8000.100776	12.133747	-0.062880	4.815404
313.862820	8000.093842	12.138752	-0.062887	4.815401
313.933577	8000.067197	12.143757	-0.062899	4.815393
313.804732	8000.076793	12.148762	-0.062875	4.815397
314.058440	8000.092731	12.153767	-0.062922	4.815400
313.939670	8000.120665	12.158771	-0.062900	4.815409
313.930960	8000.140804	12.163776	-0.062898	4.815415
314.020840	8000.136923	12.168781	-0.062914	4.815413
314.080860	8000.079103	12.173786	-0.062925	4.815396
314.068161	8000.056419	12.178791	-0.062922	4.815390
313.860546	8000.138462	12.183795	-0.062884	4.815414
313.933941	8000.076588	12.188800	-0.062897	4.815396
314.170816	8000.111488	12.193805	-0.062941	4.815405
314.061473	8000.065823	12.198810	-0.062920	4.815392
313.939110	8000.072320	12.203815	-0.062897	4.815395
314.161494	8000.085601	12.208819	-0.062938	4.815398
314.077214	8000.020043	12.213824	-0.062922	4.815379
314.172408	8000.107108	12.218829	-0.062939	4.815404
313.923032	8000.069811	12.223834	-0.062893	4.815394
313.929086	8000.138295	12.228839	-0.062894	4.815414
313.980195	8000.141254	12.233843	-0.062903	4.815415
314.113439	8000.076096	12.238848	-0.062927	4.815395
314.003486	8000.069971	12.243853	-0.062907	4.815394
313.914097	8000.064187	12.248858	-0.062890	4.815393
314.125886	8000.028123	12.253863	-0.062929	4.815381
314.321302	8000.111505	12.258867	-0.062965	4.815404
314.191949	8000.056958	12.263872	-0.062940	4.815389
314.109057	8000.058764	12.268877	-0.062925	4.815390
314.035739	8000.132345	12.273882	-0.062911	4.815412
314.012273	8000.072071	12.278887	-0.062906	4.815395
314.052091	8000.149666	12.283891	-0.062913	4.815417
314.109820	8000.102497	12.288896	-0.062924	4.815403
314.243221	8000.157059	12.293901	-0.062948	4.815418
314.113007	8000.138840	12.298906	-0.062924	4.815414
313.902993	8000.090438	12.303911	-0.062884	4.815400
313.949383	8000.109352	12.308915	-0.062893	4.815406
314.044439	8000.011494	12.313920	-0.062910	4.815377
314.086588	8000.036752	12.318925	-0.062918	4.815384
314.130984	8000.109078	12.323930	-0.062926	4.815405
314.017550	8000.064415	12.328935	-0.062904	4.815392
313.902160	8000.122334	12.333939	-0.062882	4.815410
313.734173	7999.975222	12.338944	-0.062851	4.815368
313.966212	8000.006834	12.343949	-0.062894	4.815376
313.856443	8000.038123	12.348954	-0.062873	4.815385
314.140296	7999.989358	12.353959	-0.062926	4.815370
314.346291	8000.088949	12.358963	-0.062964	4.815398
314.230497	8000.015386	12.363968	-0.062942	4.815377
314.077544	8000.064131	12.368973	-0.062913	4.815392
314.174445	8000.082814	12.373978	-0.062931	4.815397
314.123648	8000.054154	12.378983	-0.062921	4.815389
314.128613	8000.082002	12.383987	-0.062922	4.815397
314.320863	8000.022098	12.388992	-0.062957	4.815379
314.461404	8000.057539	12.393997	-0.062983	4.815388
314.176419	8000.036753	12.399002	-0.062930	4.815384
314.055201	8000.007995	12.404007	-0.062907	4.815376
314.102489	8000.137021	12.409011	-0.062915	4.815413
313.949540	8000.050016	12.414016	-0.062886	4.815389
314.016603	8000.120580	12.419021	-0.062899	4.815409
314.165508	8000.041786	12.424026	-0.062926	4.815385
314.112668	8000.020575	12.429031	-0.062916	4.815379
314.038186	8000.127273	12.434035	-0.062902	4.815411
313.886838	8000.084119	12.439040	-0.062873	4.815399
314.162372	8000.076903	12.444045	-0.062924	4.815395
314.017214	8000.076608	12.449050	-0.062897	4.815396
314.105983	8000.008575	12.454055	-0.062913	4.815376
314.282821	8000.085235	12.459059	-0.062946	4.815397
314.343616	8000.068046	12.464064	-0.062957	4.815392
314.390870	8000.057045	12.469069	-0.062965	4.815389
314.221285	8000.052069	12.474074	-0.062934	4.815388
314.255071	8000.026950	12.479079	-0.062940	4.815380
314.299818	8000.043699	12.484083	-0.062948	4.815385
314.168331	7999.977359	12.489088	-0.062923	4.815366
314.123178	8000.042856	12.494093	-0.062914	4.815386
314.323863	8000.065397	12.499098	-0.062951	4.815391
314.171352	8000.017949	12.504103	-0.062922	4.815378
314.246169	8000.126053	12.509107	-0.062936	4.815409
314.228844	8000.070157	12.514112	-0.062933	4.815393
314.237525	8000.084170	12.519117	-0.062934	4.815397
314.262026	8000.024692	12.524122	-0.062938	4.815380
314.250734	8000.011652	12.529127	-0.062936	4.815376
314.440357	8000.103489	12.534131	-0.062971	4.815402
314.211695	8000.023779	12.539136	-0.062928	4.815380
314.391243	8000.052383	12.544141	-0.062961	4.815387
314.252900	7999.998756	12.549146	-0.062935	4.815372
314.228390	7999.967326	12.554151	-0.062930	4.815363
314.207862	8000.025748	12.559155	-0.062926	4.815380
314.261138	8000.015917	12.564160	-0.062936	4.815377
314.210820	8000.059950	12.569165	-0.062926	4.815390
314.191976	8000.101299	12.574170	-0.062922	4.815403
314.243961	8000.078618	12.579175	-0.062932	4.815396
314.368934	8000.138386	12.584179	-0.062955	4.815413
314.170791	8000.081628	12.589184	-0.062917	4.815397
314.171973	8000.142549	12.594189	-0.062917	4.815415
314.114743	8000.133023	12.599194	-0.062906	4.815412
314.148315	8000.131416	12.604199	-0.062912	4.815412
314.391012	8000.186722	12.609203	-0.062957	4.815427
314.137957	8000.092711	12.614208	-0.062910	4.815400
314.201727	8000.078778	12.619213	-0.062921	4.815396
314.097863	8000.047100	12.624218	-0.062902	4.815387
314.260708	8000.027327	12.629223	-0.062932	4.815381
314.116284	8000.086903	12.634227	-0.062905	4.815399
314.086131	8000.043621	12.639232	-0.062899	4.815386
314.186591	8000.048467	12.644237	-0.062917	4.815387
314.134290	8000.067882	12.649242	-0.062907	4.815393
314.064916	8000.010055	12.654247	-0.062894	4.815377
314.143352	8000.117150	12.659251	-0.062908	4.815408
314.164016	8000.083261	12.664256	-0.062912	4.815398
314.205253	8000.062541	12.669261	-0.062919	4.815391
314.106415	8000.091874	12.674266	-0.062900	4.815400
314.259212	8000.001387	12.679271	-0.062929	4.815373
314.249485	8000.095263	12.684275	-0.062927	4.815401
314.301754	8000.081139	12.689280	-0.062936	4.815396
314.182194	8000.080199	12.694285	-0.062913	4.815397
314.327836	8000.065485	12.699290	-0.062940	4.815392
314.243698	8000.056582	12.704295	-0.062924	4.815390
314.139187	8000.134990	12.709299	-0.062905	4.815413
314.089722	8000.062528	12.714304	-0.062895	4.815392
314.097348	8000.086144	12.719309	-0.062896	4.815399
313.913139	8000.075581	12.724314	-0.062862	4.815397
314.025398	7999.995111	12.729319	-0.062882	4.815373
314.224070	8000.091373	12.734323	-0.062919	4.815400
314.248208	8000.090678	12.739328	-0.062923	4.815399
314.453163	8000.075879	12.744333	-0.062961	4.815394
314.488629	8000.079648	12.749338	-0.062967	4.815395
314.364039	8000.018766	12.754343	-0.062944	4.815378
314.441937	8000.107682	12.759347	-0.062958	4.815404
314.397135	8000.042778	12.764352	-0.062949	4.815385
314.590770	8000.066272	12.769357	-0.062985	4.815391
314.466745	8000.098395	12.774362	-0.062962	4.815401
314.444825	8000.060593	12.779367	-0.062957	4.815390
314.694790	8000.075401	12.784371	-0.063004	4.815393
314.409603	8000.052474	12.789376	-0.062950	4.815388
314.541275	8000.062114	12.794381	-0.062974	4.815390
314.493809	8000.092299	12.799386	-0.062965	4.815399
314.524814	8000.038273	12.804391	-0.062971	4.815383
314.344844	8000.073743	12.809395	-0.062937	4.815394
314.366317	8000.040937	12.814400	-0.062941	4.815385
314.632614	7999.992950	12.819405	-0.062990	4.815369
314.584239	7999.991053	12.824410	-0.062981	4.815369
314.573145	7999.973740	12.829415	-0.062978	4.815364
314.581299	8000.056155	12.834419	-0.062979	4.815388
314.443083	8000.033528	12.839424	-0.062953	4.815382
314.186855	8000.007875	12.844429	-0.062905	4.815376
314.249951	8000.066616	12.849434	-0.062917	4.815393
314.287246	8000.049037	12.854439	-0.062924	4.815387
314.333060	8000.082906	12.859443	-0.062932	4.815397
314.379405	8000.024859	12.864448	-0.062940	4.815380
314.477750	8000.072426	12.869453	-0.062958	4.815393
314.394642	8000.068884	12.874458	-0.062942	4.815393
314.470087	8000.027353	12.879463	-0.062956	4.815380
314.476063	8000.148212	12.884467	-0.062957	4.815415
314.546078	8000.071317	12.889472	-0.062970	4.815393
314.482007	8000.100157	12.894477	-0.062957	4.815401
314.461098	8000.080544	12.899482	-0.062953	4.815396
314.581766	8000.075037	12.904487	-0.062975	4.815394
314.470586	8000.090269	12.909491	-0.062954	4.815399
314.386710	8000.036476	12.914496	-0.062939	4.815383
314.621627	8000.106617	12.919501	-0.062982	4.815403
314.515353	8000.074899	12.924506	-0.062962	4.815394
314.344905	8000.062427	12.929511	-0.062930	4.815391
314.554901	8000.111846	12.934515	-0.062969	4.815404
314.377910	8000.104609	12.939520	-0.062935	4.815403
314.309442	8000.020073	12.944525	-0.062922	4.815379
314.283791	8000.045275	12.949530	-0.062917	4.815386
314.248222	8000.044659	12.954535	-0.062910	4.815386
314.449929	8000.029806	12.959539	-0.062948	4.815381
314.352558	8000.036717	12.964544	-0.062929	4.815384
314.485026	8000.043163	12.969549	-0.062954	4.815385
314.427187	8000.095623	12.974554	-0.062943	4.815400
314.435015	8000.039075	12.979559	-0.062944	4.815384
314.522417	8000.106770	12.984563	-0.062960	4.815403
314.550544	8000.074074	12.989568	-0.062965	4.815394
314.534866	8000.124026	12.994573	-0.062961	4.815408
314.383144	8000.090486	12.999578	-0.062933	4.815399
314.513824	8000.039182	13.004583	-0.062957	4.815384
314.434031	8000.068830	13.009587	-0.062942	4.815393
314.568364	8000.021862	13.014592	-0.062966	4.815378
314.416837	8000.052459	13.019597	-0.062938	4.815388
314.614191	8000.076015	13.024602	-0.062974	4.815394
314.439641	8000.037821	13.029607	-0.062942	4.815384
314.486816	8000.094160	13.034611	-0.062950	4.815400
314.448882	8000.065713	13.039616	-0.062943	4.815392
314.378947	8000.078423	13.044621	-0.062929	4.815396
314.552238	8000.113338	13.049626	-0.062961	4.815405
314.390812	8000.030467	13.054631	-0.062931	4.815382
314.418864	8000.108936	13.059635	-0.062936	4.815404
314.277782	8000.096950	13.064640	-0.062909	4.815402
314.475062	8000.067059	13.069645	-0.062946	4.815392
314.525014	8000.108480	13.074650	-0.062955	4.815404
314.290046	8000.034010	13.079655	-0.062911	4.815383
314.281647	8000.092634	13.084659	-0.062909	4.815400
314.310706	8000.040713	13.089664	-0.062914	4.815385
314.323919	8000.077249	13.094669	-0.062916	4.815396
314.293021	8000.097020	13.099674	-0.062910	4.815402
314.387897	8000.042984	13.104679	-0.062928	4.815385
314.473702	8000.073241	13.109683	-0.062943	4.815394
314.563792	8000.099293	13.114688	-0.062960	4.815401
314.668829	8000.068941	13.119693	-0.062979	4.815392
314.599155	8000.096620	13.124698	-0.062966	4.815400
314.422977	8000.111844	13.129703	-0.062933	4.815405
314.483842	8000.119241	13.134707	-0.062944	4.815407
314.591978	8000.056873	13.139712	-0.062964	4.815389
314.560402	8000.098011	13.144717	-0.062957	4.815401
314.482986	8000.077461	13.149722	-0.062943	4.815395
314.379054	8000.065022	13.154727	-0.062923	4.815392
314.580660	8000.131405	13.159731	-0.062960	4.815410
314.274662	8000.096375	13.164736	-0.062903	4.815402
314.479378	8000.082641	13.169741	-0.062941	4.815397
314.362037	8000.113805	13.174746	-0.062919	4.815406
314.341745	8000.037550	13.179751	-0.062915	4.815384
314.426977	8000.104140	13.184755	-0.062930	4.815403
314.417886	8000.061207	13.189760	-0.062928	4.815391
314.635891	8000.105415	13.194765	-0.062968	4.815403
314.230445	8000.107217	13.199770	-0.062893	4.815405
314.365990	8000.088060	13.204775	-0.062918	4.815399
314.688726	8000.075214	13.209779	-0.062977	4.815394
314.447745	8000.049814	13.214784	-0.062932	4.815387
314.586748	8000.068126	13.219789	-0.062958	4.815392
314.372475	8000.106234	13.224794	-0.062918	4.815404
314.345465	8000.063004	13.229799	-0.062912	4.815392
314.342422	8000.111028	13.234803	-0.062911	4.815406
314.443540	8000.092369	13.239808	-0.062930	4.815400
314.694333	8000.117880	13.244813	-0.062976	4.815406
314.535455	8000.077807	13.249818	-0.062947	4.815395
314.591471	8000.078710	13.254823	-0.062957	4.815395
314.724916	8000.053105	13.259827	-0.062981	4.815387
314.626946	8000.043972	13.264832	-0.062963	4.815385
314.685503	8000.067364	13.269837	-0.062973	4.815391
314.738284	8000.123796	13.274842	-0.062983	4.815408
314.578120	8000.099736	13.279847	-0.062953	4.815401
314.726531	8000.117136	13.284851	-0.062980	4.815406
314.618917	8000.108911	13.289856	-0.062960	4.815404
314.585265	8000.114741	13.294861	-0.062953	4.815406
314.525172	8000.084857	13.299866	-0.062942	4.815397
314.395025	8000.047400	13.304871	-0.062917	4.815387
314.639347	8000.072803	13.309875	-0.062962	4.815393
314.524802	8000.076222	13.314880	-0.062941	4.815395
314.543696	8000.061544	13.319885	-0.062944	4.815390
314.660567	8000.123315	13.324890	-0.062965	4.815408
314.685265	8000.029634	13.329895	-0.062970	4.815380
314.531290	8000.003539	13.334899	-0.062941	4.815374
314.427618	8000.081962	13.339904	-0.062921	4.815397
314.565966	8000.047887	13.344909	-0.062947	4.815386
314.513496	8000.100436	13.349914	-0.062937	4.815402
314.430249	8000.069100	13.354919	-0.062921	4.815393
314.396772	8000.159376	13.359923	-0.062914	4.815420
314.252995	8000.108865	13.364928	-0.062887	4.815406
314.527065	8000.078109	13.369933	-0.062938	4.815395
314.654789	8000.078063	13.374938	-0.062961	4.815395
314.601122	8000.061113	13.379943	-0.062951	4.815390
314.577345	8000.089553	13.384947	-0.062946	4.815399
314.703845	8000.027490	13.389952	-0.062970	4.815380
314.834996	7999.998641	13.394957	-0.062994	4.815371
314.605212	8000.097419	13.399962	-0.062951	4.815401
314.543700	8000.008723	13.404967	-0.062939	4.815375
314.578492	8000.115095	13.409971	-0.062945	4.815406
314.528186	8000.088581	13.414976	-0.062935	4.815399
314.628949	8000.089157	13.419981	-0.062954	4.815398
314.566102	8000.112674	13.424986	-0.062942	4.815405
314.484958	8000.034341	13.429991	-0.062927	4.815383
314.471949	8000.152747	13.434995	-0.062924	4.815418
314.559044	8000.076135	13.440000	-0.062940	4.815395
314.682819	8000.096333	13.445005	-0.062963	4.815400
314.653961	8000.109724	13.450010	-0.062957	4.815404
314.423952	8000.048163	13.455015	-0.062914	4.815387
314.522638	8000.058324	13.460019	-0.062932	4.815390
314.422149	8000.095112	13.465024	-0.062913	4.815401
314.370563	8000.082473	13.470029	-0.062903	4.815398
314.627624	8000.105950	13.475034	-0.062950	4.815403
314.512918	8000.058059	13.480039	-0.062929	4.815390
314.621121	8000.118616	13.485043	-0.062949	4.815407
314.436474	8000.068497	13.490048	-0.062914	4.815393
314.463953	8000.071064	13.495053	-0.062919	4.815394
314.461123	8000.065646	13.500058	-0.062918	4.815392
314.550584	8000.046794	13.505063	-0.062934	4.815386
314.576349	8000.074987	13.510067	-0.062939	4.815395
314.515066	8000.040809	13.515072	-0.062927	4.815385
314.438656	8000.002104	13.520077	-0.062913	4.815374
314.634372	8000.089766	13.525082	-0.062949	4.815399
314.794793	8000.059264	13.530087	-0.062978	4.815389
314.897008	8000.109034	13.535091	-0.062997	4.815403
314.794390	8000.132960	13.540096	-0.062978	4.815410
314.719264	8000.071829	13.545101	-0.062963	4.815393
314.794590	8000.094430	13.550106	-0.062977	4.815399
314.537669	8000.079454	13.555111	-0.062929	4.815396
314.843980	8000.111230	13.560115	-0.062986	4.815404
314.876463	8000.083951	13.565120	-0.062992	4.815396
314.778763	8000.050238	13.570125	-0.062973	4.815386
314.672380	8000.109375	13.575130	-0.062953	4.815404
314.646006	8000.064018	13.580135	-0.062948	4.815391
314.741815	8000.050615	13.585139	-0.062965	4.815387
314.618524	8000.082750	13.590144	-0.062942	4.815397
314.861730	8000.052551	13.595149	-0.062987	4.815387
314.815986	8000.069938	13.600154	-0.062978	4.815392
314.629164	8000.019782	13.605159	-0.062943	4.815378
314.599980	8000.111198	13.610163	-0.062937	4.815405
314.589769	8000.081073	13.615168	-0.062935	4.815396
314.698567	8000.068955	13.620173	-0.062955	4.815392
314.726488	8000.132458	13.625178	-0.062960	4.815411
314.588632	8000.059598	13.630183	-0.062934	4.815390
314.839076	8000.109688	13.635187	-0.062980	4.815404
314.636664	8000.135165	13.640192	-0.062942	4.815412
314.691193	8000.126423	13.645197	-0.062952	4.815409
314.627190	8000.173437	13.650202	-0.062940	4.815423
314.490883	8000.062122	13.655207	-0.062914	4.815391
314.570135	8000.093339	13.660211	-0.062929	4.815400
314.557245	8000.155096	13.665216	-0.062926	4.815418
314.571562	8000.100793	13.670221	-0.062929	4.815402
314.683309	8000.136825	13.675226	-0.062949	4.815412
314.520394	8000.097754	13.680231	-0.062918	4.815402
314.559826	8000.053488	13.685235	-0.062925	4.815389
314.591565	8000.081779	13.690240	-0.062931	4.815397
314.885915	8000.057774	13.695245	-0.062986	4.815388
314.849268	8000.073173	13.700250	-0.062979	4.815393
314.820147	8000.049148	13.705255	-0.062973	4.815386
314.956018	8000.086649	13.710259	-0.062998	4.815396
314.800917	8000.082982	13.715264	-0.062969	4.815396
314.862774	7999.986711	13.720269	-0.062980	4.815368
314.936071	8000.057379	13.725274	-0.062993	4.815388
314.917594	8000.001464	13.730279	-0.062989	4.815372
314.809003	8000.010326	13.735283	-0.062969	4.815375
314.636871	8000.052340	13.740288	-0.062937	4.815388
314.801737	8000.068943	13.745293	-0.062967	4.815392
314.862899	8000.163995	13.750298	-0.062978	4.815419
314.803962	8000.050756	13.755303	-0.062967	4.815387
314.829727	8000.086431	13.760307	-0.062971	4.815397
314.644302	8000.086537	13.765312	-0.062937	4.815398
314.704459	8000.026581	13.770317	-0.062947	4.815380
314.825271	8000.092692	13.775322	-0.062970	4.815399
314.922924	8000.008773	13.780327	-0.062987	4.815374
315.058405	8000.060163	13.785331	-0.063012	4.815388
314.846798	8000.078006	13.790336	-0.062973	4.815395
314.887027	8000.038028	13.795341	-0.062980	4.815383
314.958203	8000.101179	13.800346	-0.062993	4.815401
314.801728	7999.980979	13.805351	-0.062963	4.815366
314.826966	8000.085055	13.810355	-0.062968	4.815397
314.951347	8000.126641	13.815360	-0.062991	4.815408
314.923701	8000.055608	13.820365	-0.062985	4.815388
314.686971	8000.050588	13.825370	-0.062941	4.815387
314.697722	7999.997295	13.830375	-0.062943	4.815372
314.798593	8000.041697	13.835379	-0.062961	4.815384
314.777724	8000.040256	13.840384	-0.062957	4.815384
314.829739	7999.994061	13.845389	-0.062966	4.815370
314.918968	8000.116301	13.850394	-0.062983	4.815405
314.706949	8000.057175	13.855399	-0.062943	4.815389
314.850776	8000.119393	13.860403	-0.062969	4.815407
314.823208	8000.108221	13.865408	-0.062964	4.815404
314.765952	8000.106176	13.870413	-0.062953	4.815403
314.696952	8000.128522	13.875418	-0.062940	4.815410
314.724128	8000.023124	13.880423	-0.062945	4.815379
314.997645	8000.105664	13.885427	-0.062995	4.815402
314.853992	8000.124634	13.890432	-0.062968	4.815408
314.768551	8000.016300	13.895437	-0.062952	4.815377
314.727070	8000.073307	13.900442	-0.062944	4.815394
314.704359	8000.014115	13.905447	-0.062939	4.815377
314.668136	8000.043417	13.910451	-0.062932	4.815385
314.878087	8000.030839	13.915456	-0.062971	4.815381
314.681254	7999.996551	13.920461	-0.062934	4.815372
314.802994	8000.111847	13.925466	-0.062957	4.815405
314.768746	8000.040705	13.930471	-0.062950	4.815384
314.765541	8000.052384	13.935475	-0.062949	4.815388
314.789892	8000.110482	13.940480	-0.062953	4.815404
314.741629	8000.091484	13.945485	-0.062944	4.815399
314.640164	8000.085500	13.950490	-0.062925	4.815398
314.681509	8000.011336	13.955495	-0.062932	4.815376
314.716103	8000.062122	13.960499	-0.062938	4.815391
314.782189	8000.067467	13.965504	-0.062950	4.815392
314.795017	8000.056965	13.970509	-0.062953	4.815389
314.635163	8000.101320	13.975514	-0.062923	4.815403
314.587045	8000.085531	13.980519	-0.062913	4.815398
314.838942	8000.109991	13.985523	-0.062960	4.815404
314.730830	8000.124206	13.990528	-0.062939	4.815409
314.628826	8000.077594	13.995533	-0.062920	4.815396
314.726101	8000.139040	14.000538	-0.062938	4.815413
314.597534	8000.024647	14.005543	-0.062914	4.815380
314.598783	8000.021435	14.010547	-0.062914	4.815380
314.547582	8000.085763	14.015552	-0.062904	4.815399
314.798060	8000.058891	14.020557	-0.062950	4.815390
314.868057	8000.136987	14.025562	-0.062963	4.815412
314.926059	8000.019274	14.030567	-0.062973	4.815377
315.022462	8000.052914	14.035571	-0.062991	4.815387
314.992795	8000.005364	14.040576	-0.062985	4.815373
314.807261	8000.043948	14.045581	-0.062950	4.815385
314.766250	8000.100963	14.050586	-0.062943	4.815402
314.900635	8000.031549	14.055591	-0.062967	4.815381
315.056565	8000.093967	14.060595	-0.062996	4.815399
314.996330	8000.082253	14.065600	-0.062984	4.815395
314.950526	8000.049400	14.070605	-0.062976	4.815386
314.880864	8000.103802	14.075610	-0.062962	4.815402
314.716159	8000.029428	14.080615	-0.062931	4.815381
315.013485	8000.090984	14.085619	-0.062986	4.815398
315.067415	8000.118575	14.090624	-0.062996	4.815406
314.913149	8000.115990	14.095629	-0.062967	4.815406
314.922743	8000.123606	14.100634	-0.062969	4.815408
314.948718	8000.024602	14.105639	-0.062973	4.815379
314.858518	8000.093628	14.110643	-0.062956	4.815399
314.652640	8000.061327	14.115648	-0.062918	4.815391
314.873833	7999.995490	14.120653	-0.062958	4.815371
314.956479	8000.112276	14.125658	-0.062974	4.815404
314.850037	8000.061315	14.130663	-0.062953	4.815390
314.920666	8000.056047	14.135667	-0.062966	4.815388
314.896242	8000.089821	14.140672	-0.062961	4.815398
314.899811	8000.037477	14.145677	-0.062962	4.815383
314.994718	8000.117055	14.150682	-0.062979	4.815406
314.954145	8000.049015	14.155687	-0.062971	4.815386
314.860722	8000.065611	14.160691	-0.062954	4.815391
314.699506	8000.050085	14.165696	-0.062923	4.815388
314.750675	8000.073354	14.170701	-0.062933	4.815394
314.801717	8000.117999	14.175706	-0.062942	4.815407
314.628517	8000.068070	14.180711	-0.062909	4.815393
314.870780	8000.112679	14.185715	-0.062954	4.815405
314.963018	8000.048979	14.190720	-0.062971	4.815386
315.058220	8000.044118	14.195725	-0.062988	4.815384
314.996099	8000.129643	14.200730	-0.062977	4.815409
315.035161	8000.108887	14.205735	-0.062983	4.815403
315.077427	8000.101010	14.210739	-0.062991	4.815401
314.818672	8000.108451	14.215744	-0.062943	4.815404
314.828087	8000.025207	14.220749	-0.062944	4.815380
314.965687	8000.100148	14.225754	-0.062969	4.815401
314.819200	8000.052798	14.230759	-0.062942	4.815388
314.864857	8000.094148	14.235763	-0.062950	4.815400
315.066957	8000.086784	14.240768	-0.062987	4.815397
314.860629	8000.063027	14.245773	-0.062949	4.815391
314.861051	8000.086524	14.250778	-0.062948	4.815398
314.751207	8000.026955	14.255783	-0.062928	4.815381
314.884727	8000.039832	14.260787	-0.062952	4.815384
314.668352	8000.102490	14.265792	-0.062912	4.815403
314.673922	7999.119195	14.270797	-0.062912	4.815116
314.671340	7996.026198	14.275802	-0.062909	4.814213
314.519917	7990.540363	14.280807	-0.062877	4.812610
314.755806	7983.895479	14.285811	-0.062916	4.810667
314.694120	7976.641093	14.290816	-0.062900	4.808546
314.565815	7968.958927	14.295821	-0.062870	4.806299
314.535993	7961.223299	14.300826	-0.062860	4.804035
314.590787	7953.316778	14.305831	-0.062864	4.801719
314.577017	7945.328852	14.310835	-0.062856	4.799379
314.459989	7937.456151	14.315840	-0.062829	4.797072
314.359142	7929.376802	14.320845	-0.062805	4.794703
314.703036	7921.402695	14.325850	-0.062863	4.792362
314.408441	7913.326361	14.330855	-0.062803	4.789992
314.367071	7905.432049	14.335859	-0.062790	4.787674
314.351626	7897.376249	14.340864	-0.062781	4.785307
314.272953	7889.450971	14.345869	-0.062761	4.782977
314.283244	7881.407719	14.350874	-0.062758	4.780611
314.466329	7873.434427	14.355879	-0.062786	4.778264
314.489070	7865.419392	14.360883	-0.062785	4.775904
314.376193	7857.408658	14.365888	-0.062758	4.773545
314.496841	7849.370009	14.370893	-0.062775	4.771175
314.572187	7841.430007	14.375898	-0.062784	4.768834
314.226453	7833.398671	14.380903	-0.062714	4.766466
314.202265	7825.400819	14.385907	-0.062704	4.764105
314.165894	7817.440624	14.390912	-0.062692	4.761754
314.106348	7809.349940	14.395917	-0.062675	4.759364
313.849422	7801.432083	14.400922	-0.062622	4.757025
313.952884	7793.326103	14.405927	-0.062635	4.754627
313.886390	7785.304524	14.410931	-0.062618	4.752254
313.723231	7777.258494	14.415936	-0.062582	4.749872
313.929601	7769.309149	14.420941	-0.062615	4.747517
313.941763	7761.329985	14.425946	-0.062611	4.745152
313.847248	7753.297877	14.430951	-0.062588	4.742771
313.746467	7745.326602	14.435955	-0.062564	4.740407
313.882089	7737.365973	14.440960	-0.062584	4.738044
313.956817	7729.310907	14.445965	-0.062592	4.735652
313.712418	7721.361815	14.450970	-0.062541	4.733291
313.603082	7713.282633	14.455975	-0.062515	4.730890
313.980562	7705.330800	14.460979	-0.062580	4.728524
313.742013	7697.304731	14.465984	-0.062530	4.726136
313.742918	7689.293374	14.470989	-0.062525	4.723752
313.784790	7681.358744	14.475994	-0.062527	4.721388
313.441824	7673.300101	14.480999	-0.062458	4.718988
313.413725	7665.341539	14.486003	-0.062447	4.716615
313.385305	7657.325266	14.491008	-0.062436	4.714224
313.343753	7649.265911	14.496013	-0.062423	4.711819
313.251316	7641.283465	14.501018	-0.062400	4.709435
313.383750	7633.313105	14.506023	-0.062419	4.707054
313.569992	7625.261514	14.511027	-0.062448	4.704647
313.454157	7617.347452	14.516032	-0.062421	4.702280
313.376829	7609.307307	14.521037	-0.062401	4.699875
313.560871	7601.345069	14.526042	-0.062430	4.697491
313.471193	7593.255748	14.531047	-0.062408	4.695068
313.218604	7585.311233	14.536051	-0.062356	4.692688
312.920448	7577.219619	14.541056	-0.062294	4.690262
312.979328	7569.276014	14.546061	-0.062300	4.687879
313.099394	7561.283761	14.551066	-0.062317	4.685480
312.967129	7553.303466	14.556071	-0.062287	4.683084
313.072703	7545.297474	14.561075	-0.062301	4.680679
313.101273	7537.346030	14.566080	-0.062301	4.678289
312.905733	7529.292668	14.571085	-0.062259	4.675867
312.928350	7521.185528	14.576090	-0.062257	4.673427
312.845623	7513.086264	14.581095	-0.062236	4.670989
312.950379	7505.194186	14.586099	-0.062250	4.668612
313.010591	7497.191980	14.591104	-0.062256	4.666200
312.810058	7489.247659	14.596109	-0.062213	4.663805
312.816522	7481.302130	14.601114	-0.062209	4.661408
312.713647	7473.233089	14.606119	-0.062184	4.658972
312.696020	7465.254407	14.611123	-0.062176	4.656563
312.791984	7457.217250	14.616128	-0.062188	4.654134
312.575830	7449.192540	14.621133	-0.062142	4.651708
312.510833	7441.192175	14.626138	-0.062125	4.649288
312.526667	7433.204491	14.631143	-0.062122	4.646871
312.439797	7425.166061	14.636147	-0.062100	4.644437
312.419895	7417.283500	14.641152	-0.062091	4.642049
312.504602	7409.183860	14.646157	-0.062101	4.639594
312.461371	7401.260089	14.651162	-0.062088	4.637191
312.368961	7393.172691	14.656167	-0.062065	4.634737
312.418494	7385.182389	14.661171	-0.062069	4.632311
312.322931	7377.165219	14.666176	-0.062045	4.629876
312.262030	7369.192411	14.671181	-0.062029	4.627453
312.279388	7361.180787	14.676186	-0.062026	4.625017
312.280744	7353.182605	14.681191	-0.062021	4.622584
312.401071	7345.190780	14.686195	-0.062038	4.620151
312.175875	7337.241887	14.691200	-0.061991	4.617730
312.198956	7329.122187	14.696205	-0.061989	4.615256
312.306576	7321.160416	14.701210	-0.062004	4.612829
311.965466	7313.117901	14.706215	-0.061935	4.610375
312.083374	7305.180938	14.711219	-0.061951	4.607953
312.054908	7297.155163	14.716224	-0.061940	4.605502
311.888459	7289.180760	14.721229	-0.061904	4.603066
311.983700	7281.170616	14.726234	-0.061916	4.600617
311.728015	7273.159964	14.731239	-0.061863	4.598167
311.800982	7265.151252	14.736243	-0.061871	4.595716
311.666712	7257.145045	14.741248	-0.061841	4.593265
311.799650	7249.097916	14.746253	-0.061860	4.590800
311.869633	7241.118315	14.751258	-0.061867	4.588354
311.618749	7233.105932	14.756263	-0.061815	4.585897
311.832644	7225.147795	14.761267	-0.061850	4.583455
311.793033	7217.087678	14.766272	-0.061837	4.580980
311.800713	7209.131398	14.771277	-0.061833	4.578537
311.780238	7201.158123	14.776282	-0.061823	4.576086
311.557740	7193.142028	14.781287	-0.061776	4.573621
311.410869	7185.090548	14.786291	-0.061743	4.571144
311.638550	7177.070634	14.791296	-0.061780	4.568675
311.547124	7169.054079	14.796301	-0.061758	4.566206
311.443387	7161.156399	14.801306	-0.061733	4.563772
311.135211	7153.112956	14.806311	-0.061670	4.561292
311.326406	7145.135696	14.811315	-0.061700	4.558831
311.386379	7137.179424	14.816320	-0.061706	4.556375
311.212086	7129.118325	14.821325	-0.061668	4.553885
311.248863	7121.090011	14.826330	-0.061669	4.551404
311.173652	7113.051475	14.831335	-0.061650	4.548919
310.933857	7105.081773	14.836339	-0.061599	4.546453
311.075648	7097.080194	14.841344	-0.061620	4.543977
311.028144	7089.127306	14.846349	-0.061606	4.541514
311.045934	7081.096798	14.851354	-0.061604	4.539026
310.970750	7073.110503	14.856359	-0.061584	4.536550
311.031034	7065.117724	14.861363	-0.061590	4.534071
311.102951	7057.071908	14.866368	-0.061598	4.531574
310.945828	7049.038014	14.871373	-0.061563	4.529078
311.024285	7041.122576	14.876378	-0.061572	4.526619
310.813442	7033.084883	14.881383	-0.061528	4.524120
310.890288	7025.143021	14.886387	-0.061536	4.521650
310.783173	7017.132592	14.891392	-0.061511	4.519157
310.669832	7009.134700	14.896397	-0.061484	4.516666
310.992355	7001.068834	14.901402	-0.061539	4.514154
310.519196	6993.021560	14.906407	-0.061445	4.511644
310.594207	6985.012599	14.911411	-0.061454	4.509146
310.556325	6977.034983	14.916416	-0.061441	4.506656
310.474510	6969.019187	14.921421	-0.061420	4.504153
310.586536	6961.086144	14.926426	-0.061436	4.501675
310.517913	6953.074153	14.931431	-0.061417	4.499170
310.590834	6945.093331	14.936435	-0.061425	4.496674
310.320702	6937.026315	14.941440	-0.061370	4.494149
310.399442	6929.007532	14.946445	-0.061379	4.491638
310.677097	6921.066027	14.951450	-0.061425	4.489151
310.381641	6913.063715	14.956455	-0.061364	4.486641
310.258540	6905.077229	14.961459	-0.061336	4.484136
310.223593	6897.054590	14.966464	-0.061324	4.481618
310.162648	6889.041720	14.971469	-0.061307	4.479101
310.074207	6881.055530	14.976474	-0.061285	4.476592
310.108402	6873.009007	14.981479	-0.061286	4.474062
310.224782	6864.991933	14.986483	-0.061302	4.471541
310.207292	6857.011573	14.991488	-0.061293	4.469030
310.248681	6848.975581	14.996493	-0.061296	4.466499
310.211433	6841.041126	15.001498	-0.061283	4.463999
309.952868	6833.007790	15.006503	-0.061230	4.461466
309.828173	6825.042843	15.011507	-0.061201	4.458953
309.950627	6817.041884	15.016512	-0.061218	4.456428
310.122325	6809.006271	15.021517	-0.061245	4.453891
310.017059	6800.976651	15.026522	-0.061219	4.451353
310.014083	6793.003676	15.031527	-0.061213	4.448833
310.195448	6784.975637	15.036531	-0.061242	4.446294
309.758978	6777.022297	15.041536	-0.061155	4.443775
309.933040	6769.022209	15.046541	-0.061182	4.441242
309.911335	6761.041071	15.051546	-0.061172	4.438713
309.642046	6752.980260	15.056551	-0.061117	4.436156
309.821185	6744.959340	15.061555	-0.061144	4.433612
309.801313	6736.940832	15.066560	-0.061135	4.431067
309.789335	6728.942558	15.071565	-0.061127	4.428526
309.614343	6720.946323	15.076570	-0.061089	4.425984
309.424880	6712.953008	15.081575	-0.061049	4.423442
309.774926	6704.942666	15.086579	-0.061108	4.420895
309.541142	6696.984767	15.091584	-0.061059	4.418360
309.569172	6688.970734	15.096589	-0.061059	4.415808
309.456432	6680.987977	15.101594	-0.061032	4.413263
309.353225	6672.916751	15.106599	-0.061008	4.410689
309.577232	6664.958599	15.111603	-0.061044	4.408150
309.521632	6656.938044	15.116608	-0.061028	4.405589
309.362811	6648.977585	15.121613	-0.060993	4.403046
309.238587	6640.930424	15.126618	-0.060964	4.400473
309.092299	6632.974268	15.131623	-0.060932	4.397927
309.272426	6624.970515	15.136627	-0.060960	4.395367
309.025981	6616.969802	15.141632	-0.060908	4.392804
309.205532	6608.883777	15.146637	-0.060936	4.390214
309.305257	6600.954747	15.151642	-0.060949	4.387673
309.289193	6592.918461	15.156647	-0.060941	4.385095
309.163742	6585.012351	15.161651	-0.060912	4.382557
309.236676	6576.982933	15.166656	-0.060920	4.379979
309.101552	6568.995977	15.171661	-0.060889	4.377412
309.110521	6560.963571	15.176666	-0.060885	4.374829
308.915280	6552.944534	15.181671	-0.060844	4.372248
309.074573	6544.927583	15.186675	-0.060868	4.369668
309.002758	6536.973933	15.191680	-0.060849	4.367106
308.777536	6528.912664	15.196685	-0.060801	4.364507
308.997649	6521.026785	15.201690	-0.060837	4.361965
308.879196	6512.992396	15.206695	-0.060809	4.359372
308.770673	6504.980050	15.211699	-0.060784	4.356784
308.801827	6496.904052	15.216704	-0.060784	4.354176
308.395726	6488.844536	15.221709	-0.060703	4.351568
308.454923	6480.900278	15.226714	-0.060708	4.348999
308.425438	6472.903680	15.231719	-0.060697	4.346411
308.527048	6464.922659	15.236723	-0.060711	4.343827
308.460282	6456.941185	15.241728	-0.060693	4.341240
308.454955	6448.936260	15.246733	-0.060686	4.338645
308.498537	6440.939911	15.251738	-0.060689	4.336051
308.661748	6432.918859	15.256743	-0.060714	4.333449
308.407764	6424.916367	15.261747	-0.060661	4.330848
308.467140	6416.928304	15.266752	-0.060666	4.328252
308.513444	6408.895395	15.271757	-0.060670	4.325640
308.483007	6400.968784	15.276762	-0.060658	4.323061
308.344330	6392.918968	15.281767	-0.060627	4.320439
308.210818	6384.950630	15.286771	-0.060597	4.317842
308.215692	6376.942833	15.291776	-0.060592	4.315232
308.120107	6368.857028	15.296781	-0.060569	4.312594
308.150373	6360.869895	15.301786	-0.060569	4.309987
308.144014	6352.898000	15.306791	-0.060562	4.307384
308.134398	6344.853648	15.311795	-0.060555	4.304755
308.129744	6336.933422	15.316800	-0.060549	4.302165
308.094349	6328.881338	15.321805	-0.060536	4.299531
308.150097	6320.956912	15.326810	-0.060541	4.296937
307.952074	6312.909069	15.331815	-0.060499	4.294299
308.018167	6304.880748	15.336819	-0.060506	4.291668
307.976906	6296.910414	15.341824	-0.060493	4.289054
307.735693	6288.859586	15.346829	-0.060442	4.286410
307.808828	6280.907656	15.351834	-0.060450	4.283799
307.834679	6272.909503	15.356839	-0.060450	4.281171
307.911612	6264.913062	15.361843	-0.060458	4.278543
307.823816	6256.937117	15.366848	-0.060437	4.275918
307.770895	6248.824892	15.371853	-0.060421	4.273247
307.857016	6240.882811	15.376858	-0.060432	4.270632
307.597785	6232.867500	15.381863	-0.060378	4.267988
307.516823	6224.847831	15.386867	-0.060357	4.265343
307.468069	6216.944869	15.391872	-0.060343	4.262734
307.462680	6208.860354	15.396877	-0.060336	4.260064
307.569299	6200.945089	15.401882	-0.060351	4.257450
307.453227	6192.829245	15.406887	-0.060323	4.254766
307.251865	6184.889781	15.411891	-0.060280	4.252137
307.123942	6176.836384	15.416896	-0.060251	4.249470
307.265339	6168.850351	15.421901	-0.060272	4.246826
307.320403	6160.844349	15.426906	-0.060277	4.244173
307.049243	6152.906160	15.431911	-0.060221	4.241538
307.120920	6144.876786	15.436915	-0.060228	4.238874
307.358290	6136.903163	15.441920	-0.060267	4.236228
307.299759	6128.866852	15.446925	-0.060251	4.233557
307.165100	6120.896982	15.451930	-0.060220	4.230906
307.128372	6112.866468	15.456935	-0.060208	4.228234
307.213674	6104.859041	15.461939	-0.060218	4.225569
307.157970	6096.905769	15.466944	-0.060202	4.222919
306.870101	6088.876401	15.471949	-0.060143	4.220240
307.015170	6080.926340	15.476954	-0.060165	4.217590
306.761015	6072.882889	15.481959	-0.060112	4.214903
306.843864	6064.895222	15.486963	-0.060122	4.212236
306.942701	6056.913035	15.491968	-0.060135	4.209569
306.605306	6048.924047	15.496973	-0.060066	4.206894
306.831834	6040.896772	15.501978	-0.060103	4.204211
306.806735	6032.927093	15.506983	-0.060093	4.201542
306.665786	6024.927922	15.511987	-0.060061	4.198860
306.774410	6016.903739	15.516992	-0.060076	4.196171
306.628412	6008.820149	15.521997	-0.060043	4.193458
306.683546	6000.808909	15.527002	-0.060048	4.190769
306.408322	5992.849609	15.532007	-0.059991	4.188093
306.325722	5984.818744	15.537011	-0.059970	4.185393
306.515463	5976.882642	15.542016	-0.060000	4.182726
306.367363	5968.860535	15.547021	-0.059967	4.180024
306.283390	5960.899966	15.552026	-0.059946	4.177342
306.385237	5952.873592	15.557031	-0.059959	4.174639
306.334417	5944.864853	15.562035	-0.059944	4.171938
306.225301	5936.887325	15.567040	-0.059919	4.169244
306.123596	5928.850975	15.572045	-0.059894	4.166530
306.163319	5920.864096	15.577050	-0.059896	4.163832
306.016264	5912.887805	15.582055	-0.059863	4.161134
306.098105	5904.888644	15.587059	-0.059873	4.158428
306.237568	5896.886231	15.592064	-0.059893	4.155721
306.212556	5888.861495	15.597069	-0.059883	4.153002
306.227544	5880.853534	15.602074	-0.059880	4.150288
306.233802	5872.817074	15.607079	-0.059876	4.147562
306.156589	5864.819178	15.612083	-0.059856	4.144847
305.995349	5856.905800	15.617088	-0.059821	4.142157
305.986171	5848.863673	15.622093	-0.059813	4.139424
306.087256	5840.875244	15.627098	-0.059827	4.136708
305.829948	5832.871873	15.632103	-0.059773	4.133981
305.756480	5824.844351	15.637107	-0.059754	4.131247
305.786202	5816.833093	15.642112	-0.059754	4.128517
305.836727	5808.836439	15.647117	-0.059758	4.125791
305.787685	5800.896271	15.652122	-0.059743	4.123081
305.683329	5792.853702	15.657127	-0.059718	4.120334
305.668501	5784.883567	15.662131	-0.059710	4.117611
305.592552	5776.876266	15.667136	-0.059691	4.114872
305.264215	5768.814455	15.672141	-0.059624	4.112110
305.434555	5760.822396	15.677146	-0.059650	4.109376
305.451187	5752.801322	15.682151	-0.059648	4.106628
305.274192	5744.838500	15.687155	-0.059609	4.103896
305.403088	5736.868463	15.692160	-0.059628	4.101164
305.487726	5728.833567	15.697165	-0.059638	4.098407
305.384432	5720.869453	15.702170	-0.059613	4.095670
305.411789	5712.852983	15.707175	-0.059613	4.092914
305.518013	5704.833390	15.712179	-0.059627	4.090157
305.281673	5696.902408	15.717184	-0.059578	4.087424
305.176910	5688.841173	15.722189	-0.059553	4.084646
305.407063	5680.923443	15.727194	-0.059590	4.081921
305.324026	5672.890345	15.732199	-0.059569	4.079149
305.030613	5664.948020	15.737203	-0.059509	4.076404
305.077214	5656.897216	15.742208	-0.059512	4.073624
305.018115	5648.866093	15.747213	-0.059495	4.070847
305.041125	5640.894008	15.752218	-0.059494	4.068091
304.764308	5632.843042	15.757223	-0.059437	4.065301
304.963696	5624.882777	15.762227	-0.059469	4.062547
305.152291	5616.892256	15.767232	-0.059498	4.059780
304.897255	5608.943436	15.772237	-0.059445	4.057020
305.006131	5600.892403	15.777242	-0.059460	4.054228
304.889350	5592.896731	15.782247	-0.059433	4.051449
304.760822	5584.889130	15.787251	-0.059404	4.048665
304.648208	5576.885532	15.792256	-0.059377	4.045880
304.596875	5568.926166	15.797261	-0.059362	4.043110
304.636963	5560.917314	15.802266	-0.059364	4.040321
304.372718	5552.935027	15.807271	-0.059309	4.037536
304.555526	5544.883717	15.812275	-0.059338	4.034731
304.521310	5536.801666	15.817280	-0.059326	4.031910
304.443055	5528.787080	15.822285	-0.059306	4.029111
304.656919	5520.844906	15.827290	-0.059340	4.026339
304.399181	5512.882285	15.832295	-0.059287	4.023550
304.223055	5504.858398	15.837299	-0.059248	4.020740
304.292395	5496.882874	15.842304	-0.059256	4.017948
304.434005	5488.820611	15.847309	-0.059277	4.015125
304.338998	5480.899078	15.852314	-0.059253	4.012346
304.278964	5472.820539	15.857319	-0.059237	4.009510
304.345463	5464.908281	15.862323	-0.059244	4.006733
304.313235	5456.879812	15.867328	-0.059232	4.003911
304.128747	5448.886979	15.872333	-0.059192	4.001098
304.160646	5440.905112	15.877338	-0.059193	3.998290
304.071532	5432.901570	15.882343	-0.059171	3.995470
303.882773	5424.841859	15.887347	-0.059130	3.992627
303.826417	5416.858003	15.892352	-0.059114	3.989810
303.742169	5408.856341	15.897357	-0.059093	3.986985
303.840553	5400.868720	15.902362	-0.059105	3.984166
303.706545	5392.892236	15.907367	-0.059075	3.981345
303.764538	5384.917792	15.912371	-0.059080	3.978526
303.979168	5376.906359	15.917376	-0.059115	3.975694
303.605513	5368.865701	15.922381	-0.059040	3.972840
303.841515	5360.863785	15.927386	-0.059078	3.970008
303.619166	5352.887501	15.932391	-0.059031	3.967176
303.462725	5344.868145	15.937395	-0.058997	3.964327
303.505023	5336.924194	15.942400	-0.058999	3.961506
303.535182	5328.915350	15.947405	-0.058999	3.958660
303.651003	5320.945855	15.952410	-0.059015	3.955828
303.520105	5312.896658	15.957415	-0.058985	3.952960
303.534087	5304.854200	15.962419	-0.058982	3.950096
303.715557	5296.893448	15.967424	-0.059011	3.947261
303.458036	5288.875885	15.972429	-0.058957	3.944397
303.552840	5280.930844	15.977434	-0.058969	3.941562
303.425799	5272.947413	15.982439	-0.058940	3.938708
303.267903	5264.946917	15.987443	-0.058905	3.935845
303.378512	5256.939811	15.992448	-0.058920	3.932983
303.192993	5248.912336	15.997453	-0.058880	3.930106
303.231884	5240.976249	16.002458	-0.058882	3.927263
303.003761	5232.965348	16.007463	-0.058834	3.924387
303.073607	5224.957525	16.012467	-0.058842	3.921515
303.126334	5216.975538	16.017472	-0.058846	3.918650
303.157719	5208.930979	16.022477	-0.058846	3.915760
303.025129	5200.931121	16.027482	-0.058816	3.912881
302.949181	5192.908289	16.032487	-0.058796	3.909992
302.933961	5184.922957	16.037491	-0.058788	3.907116
302.860094	5176.942225	16.042496	-0.058769	3.904239
302.828922	5168.963467	16.047501	-0.058757	3.901360
303.010370	5160.963965	16.052506	-0.058786	3.898477
302.791652	5152.953240	16.057511	-0.058740	3.895579
302.620637	5144.928802	16.062515	-0.058702	3.892675
302.769419	5136.913412	16.067520	-0.058724	3.889779
302.644543	5128.970147	16.072525	-0.058696	3.886901
302.450256	5120.947781	16.077530	-0.058654	3.883991
302.409271	5112.973272	16.082535	-0.058641	3.881099
302.478572	5104.979048	16.087539	-0.058648	3.878200
302.495162	5096.977278	16.092544	-0.058646	3.875295
302.309615	5088.718422	16.097549	-0.058606	3.872290
302.381928	5080.784243	16.102554	-0.058614	3.869406
302.330136	5072.836107	16.107559	-0.058598	3.866513
302.190296	5064.886750	16.112563	-0.058567	3.863615
302.294470	5056.921521	16.117568	-0.058581	3.860714
302.183236	5048.927855	16.122573	-0.058555	3.857796
302.129167	5040.949114	16.127578	-0.058539	3.854883
302.182872	5032.912387	16.132583	-0.058544	3.851948
302.043884	5024.929160	16.137587	-0.058512	3.849027
302.174880	5016.935334	16.142592	-0.058531	3.846105
302.262578	5008.932051	16.147597	-0.058542	3.843177
302.191233	5000.994001	16.152602	-0.058523	3.840267
302.016625	4992.992914	16.157607	-0.058485	3.837329
301.849854	4984.990790	16.162611	-0.058449	3.834389
302.058856	4976.963417	16.167616	-0.058482	3.831445
301.974361	4968.942666	16.172621	-0.058461	3.828496
302.066849	4960.992720	16.177626	-0.058472	3.825573
302.301783	4952.996584	16.182631	-0.058511	3.822635
302.132228	4944.989045	16.187635	-0.058474	3.819682
302.035431	4937.054698	16.192640	-0.058450	3.816754
301.783861	4929.028848	16.197645	-0.058398	3.813788
301.759682	4921.020692	16.202650	-0.058388	3.810830
301.684755	4913.013276	16.207655	-0.058368	3.807870
301.638730	4904.989344	16.212659	-0.058354	3.804901
301.741891	4897.059095	16.217664	-0.058368	3.801969
301.750443	4889.033478	16.222669	-0.058364	3.798996
301.872756	4881.057958	16.227674	-0.058381	3.796042
301.888780	4873.015805	16.232679	-0.058379	3.793059
301.682851	4864.996505	16.237683	-0.058335	3.790078
301.574057	4857.046706	16.242688	-0.058309	3.787121
301.218856	4849.033113	16.247693	-0.058237	3.784134
301.675662	4841.052016	16.252698	-0.058317	3.781174
301.568843	4833.047157	16.257703	-0.058292	3.778190
301.404737	4825.039569	16.262707	-0.058256	3.775202
301.484188	4817.034548	16.267712	-0.058265	3.772217
301.395675	4809.001719	16.272717	-0.058243	3.769216
301.306435	4801.063917	16.277722	-0.058221	3.766249
301.036248	4793.065010	16.282727	-0.058165	3.763251
301.276340	4785.032175	16.287731	-0.058204	3.760251
301.294308	4777.108463	16.292736	-0.058202	3.757284
301.247454	4769.044300	16.297741	-0.058188	3.754260
301.160358	4761.025754	16.302746	-0.058166	3.751250
301.100304	4753.042770	16.307751	-0.058149	3.748252
301.170721	4745.029018	16.312755	-0.058157	3.745242
301.007851	4737.095168	16.317760	-0.058121	3.742255
300.766537	4729.080592	16.322765	-0.058071	3.739234
301.020679	4721.097841	16.327770	-0.058112	3.736233
300.631435	4713.094860	16.332775	-0.058034	3.733207
300.914382	4705.048631	16.337779	-0.058082	3.730178
300.782234	4697.087201	16.342784	-0.058052	3.727170
300.541072	4689.059081	16.347789	-0.058001	3.724130
300.596449	4681.143331	16.352794	-0.058006	3.721138
300.671864	4673.101542	16.357799	-0.058014	3.718096
300.498683	4665.104499	16.362803	-0.057977	3.715063
300.520602	4657.054595	16.367808	-0.057975	3.712012
300.629826	4649.023768	16.372813	-0.057990	3.708968
300.587925	4641.064341	16.377818	-0.057977	3.705944
300.503300	4633.087929	16.382823	-0.057956	3.702911
300.372727	4625.080885	16.387827	-0.057926	3.699862
300.681798	4617.130497	16.392832	-0.057978	3.696844
300.411607	4609.125296	16.397837	-0.057922	3.693787
300.335989	4601.158263	16.402842	-0.057902	3.690748
300.163459	4593.184591	16.407847	-0.057865	3.687701
300.264519	4585.113715	16.412851	-0.057878	3.684621
300.284465	4577.201069	16.417856	-0.057876	3.681597
300.199136	4569.164053	16.422861	-0.057855	3.678520
300.155132	4561.191368	16.427866	-0.057841	3.675466
299.913784	4553.179077	16.432871	-0.057791	3.672390
300.011511	4545.132163	16.437875	-0.057803	3.669306
299.982592	4537.183423	16.442880	-0.057793	3.666255
299.891873	4529.159378	16.447885	-0.057770	3.663170
299.801901	4521.191601	16.452890	-0.057748	3.660104
299.850310	4513.208185	16.457895	-0.057751	3.657033
299.807160	4505.171243	16.462899	-0.057738	3.653937
299.872758	4497.164487	16.467904	-0.057745	3.650852
299.792283	4489.177703	16.472909	-0.057724	3.647769
299.614671	4481.181746	16.477914	-0.057685	3.644677
299.420374	4473.244684	16.482919	-0.057644	3.641604
299.499270	4465.226177	16.487923	-0.057653	3.638505
299.761350	4457.228406	16.492928	-0.057696	3.635416
299.566771	4449.199727	16.497933	-0.057655	3.632301
299.438398	4441.222519	16.502938	-0.057625	3.629204
299.439400	4433.190891	16.507943	-0.057620	3.626087
299.402947	4425.201735	16.512947	-0.057608	3.622983
299.233820	4417.244008	16.517952	-0.057571	3.619884
299.267310	4409.249248	16.522957	-0.057571	3.616775
299.409295	4401.229664	16.527962	-0.057592	3.613655
299.140970	4393.245165	16.532967	-0.057537	3.610536
299.112632	4385.242675	16.537971	-0.057526	3.607413
299.223653	4377.289974	16.542976	-0.057541	3.604311
298.978223	4369.291233	16.547981	-0.057490	3.601179
299.139174	4361.309609	16.552986	-0.057514	3.598061
299.172111	4353.292995	16.557991	-0.057515	3.594924
298.969624	4345.293124	16.562995	-0.057472	3.591784
298.986737	4337.313964	16.568000	-0.057470	3.588655
298.940723	4329.279535	16.573005	-0.057455	3.585501
299.136995	4321.318853	16.578010	-0.057486	3.582379
298.848629	4313.341506	16.583015	-0.057427	3.579234
298.864079	4305.328556	16.588019	-0.057425	3.576081
298.966326	4297.337724	16.593024	-0.057438	3.572937
298.810025	4289.300788	16.598029	-0.057404	3.569764
298.842959	4281.359994	16.603034	-0.057404	3.566631
298.871888	4273.343492	16.608039	-0.057404	3.563466
298.668977	4265.359903	16.613043	-0.057361	3.560305
298.844370	4257.413876	16.618048	-0.057388	3.557166
298.732455	4249.352677	16.623053	-0.057362	3.553971
298.787326	4241.259606	16.628058	-0.057366	3.550765
298.624966	4233.307241	16.633063	-0.057331	3.547605
298.475044	4225.311595	16.638067	-0.057297	3.544426
298.681300	4217.357742	16.643072	-0.057330	3.541271
298.524010	4209.348777	16.648077	-0.057295	3.538081
298.284558	4201.371336	16.653082	-0.057245	3.534898
298.204466	4193.349998	16.658087	-0.057225	3.531699
298.491942	4185.326903	16.663091	-0.057273	3.528508
298.372755	4177.367623	16.668096	-0.057245	3.525327
298.289477	4169.418321	16.673101	-0.057224	3.522148
298.383939	4161.428339	16.678106	-0.057236	3.518955
298.031455	4153.476654	16.683111	-0.057165	3.515762
298.074156	4145.410138	16.688115	-0.057167	3.512531
298.189998	4137.412325	16.693120	-0.057184	3.509327
298.185860	4129.382042	16.698125	-0.057177	3.506104
298.187082	4121.414661	16.703130	-0.057172	3.502903
298.052254	4113.448039	16.708135	-0.057141	3.499695
297.976688	4105.495815	16.713139	-0.057122	3.496492
298.067119	4097.467504	16.718144	-0.057133	3.493260
297.874994	4089.456264	16.723149	-0.057092	3.490023
297.764681	4081.506452	16.728154	-0.057066	3.486811
297.773270	4073.492900	16.733159	-0.057062	3.483574
297.733963	4065.510630	16.738163	-0.057049	3.480345
297.849501	4057.562133	16.743168	-0.057065	3.477131
297.719569	4049.514013	16.748173	-0.057035	3.473867
297.527680	4041.487668	16.753178	-0.056994	3.470606
297.485826	4033.529314	16.758183	-0.056981	3.467374
297.578498	4025.504709	16.763187	-0.056993	3.464117
297.554435	4017.568298	16.768192	-0.056983	3.460889
297.425564	4009.546494	16.773197	-0.056953	3.457620
297.556339	4001.526073	16.778202	-0.056972	3.454356
297.544611	3993.546058	16.783207	-0.056964	3.451101
297.263418	3985.547899	16.788211	-0.056906	3.447827
297.419222	3977.577164	16.793216	-0.056930	3.444576
297.475573	3969.585316	16.798221	-0.056935	3.441309
297.310082	3961.644197	16.803226	-0.056899	3.438053
297.192810	3953.609279	16.808231	-0.056871	3.434757
297.138406	3945.591463	16.813235	-0.056856	3.431467
297.242192	3937.587440	16.818240	-0.056869	3.428184
297.077833	3929.584915	16.823245	-0.056833	3.424890
297.313463	3921.614218	16.828250	-0.056872	3.421619
297.136885	3913.637224	16.833255	-0.056833	3.418329
296.851668	3905.636074	16.838259	-0.056775	3.415022
296.947500	3897.651389	16.843264	-0.056787	3.411731
296.872115	3889.632639	16.848269	-0.056768	3.408418
296.770286	3881.654125	16.853274	-0.056743	3.405116
296.690693	3873.722278	16.858279	-0.056723	3.401832
296.774197	3865.689575	16.863283	-0.056733	3.398508
296.859302	3857.730807	16.868288	-0.056743	3.395212
296.695143	3849.633686	16.873293	-0.056707	3.391847
296.757186	3841.639865	16.878298	-0.056713	3.388529
296.663613	3833.667713	16.883303	-0.056690	3.385211
296.518835	3825.707000	16.888307	-0.056658	3.381893
296.634732	3817.723120	16.893312	-0.056674	3.378571
296.530327	3809.724573	16.898317	-0.056649	3.375232
296.552640	3801.734434	16.903322	-0.056648	3.371898
296.443229	3793.758939	16.908327	-0.056622	3.368562
296.538324	3785.738119	16.913331	-0.056634	3.365210
296.566539	3777.783152	16.918336	-0.056634	3.361881
296.232354	3769.797901	16.923341	-0.056566	3.358523
296.426821	3761.821458	16.928346	-0.056597	3.355184
296.395740	3753.771985	16.933351	-0.056585	3.351803
296.251952	3745.775282	16.938355	-0.056553	3.348436
296.481254	3737.786285	16.943360	-0.056590	3.345083
296.250561	3729.851035	16.948365	-0.056542	3.341733
296.181378	3721.834317	16.953370	-0.056523	3.338350
296.108022	3713.864574	16.958375	-0.056504	3.334984
295.885535	3705.837647	16.963379	-0.056457	3.331585
296.073863	3697.856111	16.968384	-0.056487	3.328217
295.939203	3689.863731	16.973389	-0.056456	3.324828
296.022136	3681.911982	16.978394	-0.056466	3.321462
296.049849	3673.920896	16.983399	-0.056466	3.318073
295.692645	3665.925661	16.988403	-0.056394	3.314665
295.781789	3657.913268	16.993408	-0.056405	3.311263
295.708813	3649.902185	16.998413	-0.056386	3.307851
295.836146	3641.869877	17.003418	-0.056404	3.304435
295.725109	3633.962199	17.008423	-0.056378	3.301059
295.776015	3625.953896	17.013427	-0.056382	3.297643
295.849540	3617.950387	17.018432	-0.056390	3.294226
295.603548	3609.969939	17.023437	-0.056339	3.290803
295.518139	3601.978385	17.028442	-0.056317	3.287379
295.572136	3593.992843	17.033447	-0.056322	3.283958
295.456577	3586.014902	17.038451	-0.056295	3.280531
295.578840	3578.053638	17.043456	-0.056312	3.277116
295.497232	3570.008776	17.048461	-0.056291	3.273654
295.344301	3562.012297	17.053466	-0.056258	3.270207
295.296901	3554.051660	17.058471	-0.056243	3.266775
295.380701	3546.031740	17.063475	-0.056253	3.263319
295.454661	3538.053701	17.068480	-0.056262	3.259877
295.178205	3530.116877	17.073485	-0.056205	3.256436
295.240656	3522.073814	17.078490	-0.056211	3.252959
295.268174	3514.063432	17.083495	-0.056210	3.249490
294.956786	3506.129536	17.088499	-0.056147	3.246037
295.105358	3498.136588	17.093504	-0.056169	3.242574
295.121084	3490.119887	17.098509	-0.056166	3.239091
294.984992	3482.177536	17.103514	-0.056136	3.235630
294.790966	3474.118009	17.108519	-0.056094	3.232113
294.808746	3466.090571	17.113523	-0.056092	3.228614
295.010122	3458.101168	17.118528	-0.056124	3.225136
295.007602	3450.140077	17.123533	-0.056118	3.221657
294.899718	3442.162505	17.128538	-0.056092	3.218164
294.855240	3434.175582	17.133543	-0.056078	3.214665
294.793324	3426.178377	17.138547	-0.056061	3.211157
294.685110	3418.204978	17.143552	-0.056036	3.207654
294.605614	3410.230530	17.148557	-0.056015	3.204148
294.628654	3402.257274	17.153562	-0.056014	3.200642
294.446251	3394.290266	17.158567	-0.055975	3.197127
294.435647	3386.258433	17.163571	-0.055967	3.193587
294.627331	3378.238873	17.168576	-0.055997	3.190056
294.351360	3370.275572	17.173581	-0.055941	3.186527
294.359343	3362.300420	17.178586	-0.055937	3.183001
294.564359	3354.303943	17.183591	-0.055969	3.179470
294.395161	3346.328960	17.188595	-0.055932	3.175928
294.280852	3338.345722	17.193600	-0.055906	3.172381
294.416654	3330.303801	17.198605	-0.055925	3.168815
294.253646	3322.341843	17.203610	-0.055889	3.165267
294.172527	3314.397088	17.208615	-0.055869	3.161727
294.096347	3306.395686	17.213619	-0.055849	3.158158
294.255710	3298.411247	17.218624	-0.055873	3.154602
293.983218	3290.382096	17.223629	-0.055817	3.151004
293.863065	3282.414372	17.228634	-0.055789	3.147435
293.799344	3274.431413	17.233639	-0.055772	3.143858
293.907884	3266.423989	17.238643	-0.055787	3.140274
293.918640	3258.472110	17.243648	-0.055783	3.136706
293.750042	3250.453154	17.248653	-0.055746	3.133096
293.815002	3242.456584	17.253658	-0.055753	3.129502
293.702619	3234.506779	17.258663	-0.055726	3.125918
293.570677	3226.531404	17.263667	-0.055696	3.122316
293.780273	3218.543886	17.268672	-0.055730	3.118721
293.574032	3210.546014	17.273677	-0.055686	3.115098
293.440120	3202.557253	17.278682	-0.055655	3.111478
293.647194	3194.541791	17.283687	-0.055689	3.107857
293.605556	3186.566612	17.288691	-0.055675	3.104239
293.568246	3178.620255	17.293696	-0.055663	3.100630
293.333903	3170.634966	17.298701	-0.055614	3.096990
293.485959	3162.649844	17.303706	-0.055637	3.093363
293.559878	3154.616129	17.308711	-0.055645	3.089707
293.287204	3146.654216	17.313715	-0.055589	3.086063
293.303854	3138.710187	17.318720	-0.055586	3.082436
293.327912	3130.685348	17.323725	-0.055585	3.078768
293.151423	3122.720402	17.328730	-0.055547	3.075114
292.989774	3114.669550	17.333735	-0.055511	3.071417
293.137704	3106.635711	17.338739	-0.055533	3.067738
293.179728	3098.679977	17.343744	-0.055535	3.064085
293.214036	3090.706008	17.348749	-0.055536	3.060419
293.202068	3082.742252	17.353754	-0.055529	3.056752
293.085082	3074.752819	17.358759	-0.055501	3.053063
292.865543	3066.759314	17.363763	-0.055455	3.049362
292.933877	3058.809438	17.368768	-0.055462	3.045692
292.920317	3050.829015	17.373773	-0.055454	3.041998
292.943311	3042.868658	17.378778	-0.055453	3.038311
292.674901	3034.901049	17.383783	-0.055398	3.034603
292.569628	3026.865926	17.388787	-0.055372	3.030866
292.806740	3018.876302	17.393792	-0.055411	3.027162
292.468292	3010.911382	17.398797	-0.055343	3.023438
292.503807	3002.906720	17.403802	-0.055344	3.019708
292.578831	2994.946577	17.408807	-0.055352	3.015997
292.469243	2986.939413	17.413811	-0.055326	3.012250
292.301847	2978.973678	17.418816	-0.055290	3.008515
292.166965	2970.969882	17.423821	-0.055259	3.004759
292.165066	2963.026022	17.428826	-0.055253	3.001033
292.313309	2955.044963	17.433831	-0.055275	2.997292
292.418082	2947.013361	17.438835	-0.055289	2.993520
292.545795	2938.992050	17.443840	-0.055307	2.989750
292.315086	2931.031393	17.448845	-0.055259	2.985986
292.308008	2923.070349	17.453850	-0.055252	2.982228
292.306210	2915.104920	17.458855	-0.055246	2.978464
292.105834	2907.100853	17.463859	-0.055204	2.974666
292.165877	2899.116821	17.468864	-0.055209	2.970886
291.887755	2891.162023	17.473869	-0.055152	2.967098
291.889726	2883.167787	17.478874	-0.055147	2.963301
291.706356	2875.222736	17.483879	-0.055107	2.959513
291.726622	2867.248349	17.488883	-0.055106	2.955716
291.822107	2859.213276	17.493888	-0.055118	2.951889
291.868230	2851.209589	17.498893	-0.055121	2.948070
291.870912	2843.236614	17.503898	-0.055116	2.944259
291.928948	2835.264705	17.508903	-0.055121	2.940445
291.792420	2827.304710	17.513907	-0.055090	2.936623
291.590052	2819.338263	17.518912	-0.055047	2.932789
291.668563	2811.302393	17.523917	-0.055056	2.928931
291.439052	2803.343764	17.528922	-0.055008	2.925089
291.416149	2795.405493	17.533927	-0.054998	2.921263
291.562575	2787.397007	17.538931	-0.055020	2.917406
291.569541	2779.390446	17.543936	-0.055016	2.913538
291.331248	2771.351184	17.548941	-0.054966	2.909637
291.260308	2763.379756	17.553946	-0.054947	2.905771
291.245293	2755.425668	17.558951	-0.054939	2.901912
291.157000	2747.464576	17.563955	-0.054917	2.898040
291.266840	2739.467216	17.568960	-0.054932	2.894157
291.077257	2731.470822	17.573965	-0.054891	2.890252
291.059595	2723.502062	17.578970	-0.054882	2.886365
290.902384	2715.575551	17.583975	-0.054848	2.882485
290.975457	2707.566491	17.588979	-0.054856	2.878573
291.086367	2699.600374	17.593984	-0.054871	2.874678
290.873476	2691.594049	17.598989	-0.054826	2.870741
290.853648	2683.615312	17.603994	-0.054817	2.866822
290.836799	2675.631298	17.608999	-0.054808	2.862895
290.718196	2667.669691	17.614003	-0.054780	2.858969
290.696855	2659.704333	17.619008	-0.054771	2.855041
290.734667	2651.694618	17.624013	-0.054772	2.851088
290.645284	2643.722989	17.629018	-0.054750	2.847142
290.724915	2635.748995	17.634023	-0.054760	2.843198
290.397117	2627.795105	17.639027	-0.054693	2.839237
290.548736	2619.822535	17.644032	-0.054716	2.835287
290.337558	2611.805641	17.649037	-0.054671	2.831289
290.411848	2603.815895	17.654042	-0.054679	2.827316
290.555680	2595.837535	17.659047	-0.054701	2.823346
290.220186	2587.874530	17.664051	-0.054633	2.819351
290.308865	2579.912458	17.669056	-0.054644	2.815375
290.423645	2571.896280	17.674061	-0.054660	2.811368
290.337308	2563.945077	17.679066	-0.054638	2.807376
290.241066	2555.972198	17.684071	-0.054615	2.803367
290.078197	2548.000470	17.689075	-0.054579	2.799349
290.136715	2540.055588	17.694080	-0.054584	2.795352
290.020284	2532.019794	17.699085	-0.054557	2.791293
290.078062	2524.031772	17.704090	-0.054562	2.787262
290.112502	2516.064769	17.709095	-0.054563	2.783234
289.811434	2508.116273	17.714099	-0.054502	2.779191
289.839404	2500.149172	17.719104	-0.054501	2.775151
289.734319	2492.142855	17.724109	-0.054476	2.771078
289.858113	2484.155956	17.729114	-0.054494	2.767022
289.767631	2476.206398	17.734119	-0.054472	2.762967
289.702235	2468.215482	17.739123	-0.054454	2.758886
289.916096	2460.259181	17.744128	-0.054488	2.754833
289.680080	2452.190606	17.749133	-0.054439	2.750690
289.620367	2444.237720	17.754138	-0.054422	2.746610
289.688189	2436.276765	17.759143	-0.054429	2.742528
289.349169	2428.340529	17.764147	-0.054361	2.738428
289.459772	2420.364935	17.769152	-0.054376	2.734329
289.533175	2412.328806	17.774157	-0.054384	2.730190
289.520876	2404.369982	17.779162	-0.054376	2.726080
289.403773	2396.436245	17.784167	-0.054349	2.721970
289.367552	2388.455523	17.789171	-0.054337	2.717834
289.561769	2380.475692	17.794176	-0.054367	2.713706
289.330683	2372.487893	17.799181	-0.054319	2.709542
289.079388	2364.540707	17.804186	-0.054267	2.705392
289.204995	2356.567224	17.809191	-0.054284	2.701244
289.397612	2348.557813	17.814195	-0.054315	2.697076
289.063783	2340.643135	17.819200	-0.054247	2.692918
289.166897	2332.621456	17.824205	-0.054261	2.688725
289.227182	2324.650719	17.829210	-0.054267	2.684549
289.059522	2316.730607	17.834215	-0.054230	2.680379
288.897157	2308.771861	17.839219	-0.054194	2.676183
289.073874	2300.754351	17.844224	-0.054222	2.671970
288.848770	2292.779291	17.849229	-0.054174	2.667747
288.681096	2284.810585	17.854234	-0.054137	2.663525
288.760262	2276.842200	17.859239	-0.054147	2.659312
288.721096	2268.849650	17.864243	-0.054134	2.655072
288.727471	2260.877243	17.869248	-0.054130	2.650839
288.611532	2252.910552	17.874253	-0.054103	2.646595
288.805292	2244.896463	17.879258	-0.054133	2.642338
288.666981	2236.989175	17.884263	-0.054102	2.638110
288.399857	2229.020898	17.889267	-0.054047	2.633833
288.265033	2221.038044	17.894272	-0.054016	2.629551
288.138359	2213.069593	17.899277	-0.053987	2.625270
288.217487	2205.089346	17.904282	-0.053996	2.620989
288.430997	2197.121394	17.909287	-0.054031	2.616717
288.295958	2189.125030	17.914291	-0.054000	2.612399
288.206240	2181.174191	17.919296	-0.053978	2.608102
287.898385	2173.226426	17.924301	-0.053915	2.603785
287.926279	2165.258540	17.929306	-0.053915	2.599472
287.965712	2157.294654	17.934311	-0.053916	2.595155
288.002681	2149.106610	17.939315	-0.053918	2.590708
287.903994	2141.181130	17.944320	-0.053894	2.586388
288.021264	2133.224134	17.949325	-0.053910	2.582058
287.938906	2125.304051	17.954330	-0.053889	2.577728
287.785306	2117.378624	17.959335	-0.053855	2.573382
287.687427	2109.394184	17.964339	-0.053832	2.569000
287.641831	2101.435013	17.969344	-0.053818	2.564628
287.576982	2093.497260	17.974349	-0.053800	2.560259
287.547476	2085.543980	17.979354	-0.053789	2.555877
287.462835	2077.572328	17.984359	-0.053768	2.551473
287.449001	2069.565425	17.989363	-0.053760	2.547047
287.662681	2061.600997	17.994368	-0.053794	2.542653
287.407190	2053.677306	17.999373	-0.053741	2.538241
287.225334	2045.726150	18.004378	-0.053702	2.533810
287.421232	2037.714988	18.009383	-0.053733	2.529366
287.390107	2029.745417	18.014387	-0.053721	2.524921
287.425672	2021.809001	18.019392	-0.053723	2.520491
287.110894	2013.877922	18.024397	-0.053659	2.516031
287.221237	2005.834410	18.029402	-0.053674	2.511531
287.203970	1997.864992	18.034407	-0.053665	2.507055
287.051102	1989.902882	18.039411	-0.053631	2.502565
287.095392	1981.965967	18.044416	-0.053634	2.498096
286.974328	1974.011544	18.049421	-0.053606	2.493597
286.843584	1966.038051	18.054426	-0.053576	2.489078
286.986331	1958.070367	18.059431	-0.053597	2.484575
286.850094	1950.116979	18.064435	-0.053566	2.480050
286.841532	1942.190384	18.069440	-0.053559	2.475543
286.813989	1934.170640	18.074445	-0.053548	2.470972
286.821620	1926.198597	18.079450	-0.053544	2.466423
287.040741	1918.236548	18.084455	-0.053580	2.461887
286.873107	1910.301489	18.089459	-0.053543	2.457329
286.711860	1902.367643	18.094464	-0.053507	2.452763
286.679535	1894.374250	18.099469	-0.053496	2.448165
286.633840	1886.413348	18.104474	-0.053482	2.443576
286.367165	1878.511353	18.109479	-0.053427	2.438995
286.576981	1870.498215	18.114483	-0.053460	2.434377
286.390057	1862.475487	18.119488	-0.053420	2.429715
286.401700	1854.510013	18.124493	-0.053417	2.425093
286.341279	1846.572196	18.129498	-0.053400	2.420472
286.438416	1838.618789	18.134503	-0.053413	2.415845
286.075405	1830.673485	18.139507	-0.053340	2.411179
285.982845	1822.726246	18.144512	-0.053317	2.406523
286.134777	1814.753919	18.149517	-0.053340	2.401863
286.052279	1806.813860	18.154522	-0.053319	2.397194
285.970632	1798.862429	18.159527	-0.053298	2.392509
285.854879	1790.887525	18.164531	-0.053271	2.387799
285.894488	1782.918454	18.169536	-0.053273	2.383095
285.855968	1774.965806	18.174541	-0.053260	2.378385
285.756057	1767.023229	18.179546	-0.053236	2.373667
285.846477	1759.042833	18.184551	-0.053248	2.368933
285.680227	1751.086683	18.189555	-0.053211	2.364183
285.706760	1743.140762	18.194560	-0.053211	2.359444
285.707205	1735.208299	18.199565	-0.053205	2.354702
285.542180	1727.231385	18.204570	-0.053169	2.349911
285.659711	1719.252332	18.209575	-0.053185	2.345131
285.316797	1711.336068	18.214579	-0.053116	2.340342
285.411277	1703.385898	18.219584	-0.053128	2.335558
285.221807	1695.416957	18.224589	-0.053087	2.330730
285.121868	1687.467401	18.229594	-0.053063	2.325911
285.288674	1679.496979	18.234599	-0.053089	2.321091
285.019890	1671.591174	18.239603	-0.053033	2.316265
285.049063	1663.602381	18.244608	-0.053033	2.311402
285.193527	1655.615604	18.249613	-0.053055	2.306540
284.969816	1647.691452	18.254618	-0.053008	2.301676
284.891598	1639.763452	18.259623	-0.052988	2.296810
284.789670	1631.798168	18.264627	-0.052963	2.291910
284.791520	1623.838476	18.269632	-0.052958	2.287011
284.825889	1615.892100	18.274637	-0.052959	2.282113
284.614494	1607.974736	18.279642	-0.052914	2.277201
284.743942	1599.951687	18.284647	-0.052933	2.272242
284.567260	1591.974374	18.289651	-0.052894	2.267275
284.460260	1584.043587	18.294656	-0.052869	2.262331
284.624581	1576.087023	18.299661	-0.052894	2.257384
284.533469	1568.145362	18.304666	-0.052872	2.252414
284.356953	1560.225454	18.309671	-0.052833	2.247438
284.483852	1552.242137	18.314675	-0.052851	2.242438
284.593673	1544.302705	18.319680	-0.052866	2.237453
284.289403	1536.393509	18.324685	-0.052804	2.232440
284.380951	1528.405165	18.329690	-0.052816	2.227400
284.562456	1520.449539	18.334695	-0.052844	2.222377
284.317676	1512.541877	18.339699	-0.052793	2.217336
284.259613	1504.596456	18.344704	-0.052777	2.212276
284.221323	1496.638093	18.349709	-0.052764	2.207197
284.167889	1488.709952	18.354714	-0.052749	2.202125
284.315627	1480.768541	18.359719	-0.052771	2.197051
284.164434	1472.806747	18.364723	-0.052737	2.191925
284.258405	1464.837451	18.369728	-0.052749	2.186804
283.928478	1456.945608	18.374733	-0.052682	2.181683
284.029466	1448.984840	18.379738	-0.052696	2.176544
283.893627	1441.044928	18.384743	-0.052665	2.171385
283.679328	1433.111376	18.389747	-0.052620	2.166210
283.590029	1425.190838	18.394752	-0.052598	2.161043
283.782715	1417.228995	18.399757	-0.052628	2.155863
283.801102	1409.252903	18.404762	-0.052626	2.150645
283.648922	1401.340981	18.409767	-0.052592	2.145440
283.556762	1393.399211	18.414771	-0.052569	2.140209
283.544985	1385.485718	18.419776	-0.052562	2.134991
283.497735	1377.527295	18.424781	-0.052548	2.129727
283.519446	1369.581940	18.429786	-0.052546	2.124466
283.398400	1361.696985	18.434791	-0.052518	2.119217
283.273725	1353.748792	18.439795	-0.052489	2.113914
283.108571	1345.756393	18.444800	-0.052453	2.108563
283.094612	1337.807255	18.449805	-0.052445	2.103242
283.113645	1329.886228	18.454810	-0.052443	2.097930
282.984495	1321.973797	18.459815	-0.052414	2.092596
282.896261	1314.010709	18.464819	-0.052392	2.087218
282.885040	1306.102888	18.469824	-0.052384	2.081871
282.784019	1298.185429	18.474829	-0.052360	2.076494
282.888686	1290.214273	18.479834	-0.052374	2.071088
282.919654	1282.288544	18.484839	-0.052374	2.065691
282.597302	1274.380799	18.489843	-0.052309	2.060257
282.722078	1266.450111	18.494848	-0.052327	2.054838
282.708116	1258.494721	18.499853	-0.052319	2.049373
282.783990	1250.561169	18.504858	-0.052327	2.043918
282.727948	1242.666966	18.509863	-0.052311	2.038462
282.464730	1234.750304	18.514867	-0.052257	2.032955
282.646451	1226.770203	18.519872	-0.052285	2.027434
282.604482	1218.844886	18.524877	-0.052272	2.021914
282.439209	1210.946254	18.529882	-0.052236	2.016384
282.441466	1203.012772	18.534887	-0.052231	2.010832
282.415241	1195.072740	18.539891	-0.052220	2.005257
282.228156	1187.193473	18.544896	-0.052180	1.999692
282.139954	1179.281162	18.549901	-0.052158	1.994099
282.125273	1171.313869	18.554906	-0.052150	1.988459
282.263225	1163.391257	18.559911	-0.052170	1.982850
281.910257	1155.510418	18.564915	-0.052099	1.977204
282.044660	1147.561507	18.569920	-0.052119	1.971544
282.014028	1139.638164	18.574925	-0.052107	1.965869
281.917167	1131.737184	18.579930	-0.052084	1.960186
281.790485	1123.853241	18.584935	-0.052055	1.954496
281.795448	1115.849982	18.589939	-0.052050	1.948717
281.755885	1107.948568	18.594944	-0.052038	1.942990
281.681058	1100.032195	18.599949	-0.052018	1.937231
281.703904	1092.106718	18.604954	-0.052017	1.931460
281.705664	1084.187797	18.609959	-0.052012	1.925673
281.509602	1076.298474	18.614963	-0.051970	1.919869
281.578770	1068.394758	18.619968	-0.051977	1.914066
281.569638	1060.451522	18.624973	-0.051970	1.908207
281.453962	1052.559123	18.629978	-0.051943	1.902356
281.390383	1044.670353	18.634983	-0.051926	1.896496
281.166789	1036.757627	18.639987	-0.051879	1.890581
281.313663	1028.823502	18.644992	-0.051901	1.884674
281.163812	1020.949701	18.649997	-0.051867	1.878760
281.138534	1013.031180	18.655002	-0.051857	1.872807
281.257389	1005.093281	18.660007	-0.051874	1.866838
281.115763	997.197359	18.665011	-0.051842	1.860851
281.066786	989.305772	18.670016	-0.051827	1.854859
281.100478	981.380540	18.675021	-0.051828	1.848831
281.006161	973.486233	18.680026	-0.051805	1.842792
281.081884	965.595798	18.685031	-0.051814	1.836757
280.976092	957.686517	18.690035	-0.051789	1.830665
280.760462	949.826391	18.695040	-0.051743	1.824578
280.471586	941.965067	18.700045	-0.051684	1.818461
280.715926	934.005951	18.705050	-0.051724	1.812311
280.763281	926.106834	18.710055	-0.051727	1.806164
280.389640	918.256611	18.715059	-0.051652	1.799982
280.420662	910.360625	18.720064	-0.051653	1.793793
280.218483	902.422469	18.725069	-0.051610	1.787520
280.139816	894.532792	18.730074	-0.051590	1.781279
280.203918	886.646823	18.735079	-0.051596	1.775036
280.000369	878.763167	18.740083	-0.051553	1.768740
280.110327	870.859634	18.745088	-0.051568	1.762444
279.933629	863.006566	18.750093	-0.051529	1.756131
279.858959	855.097695	18.755098	-0.051510	1.749762
280.031938	847.190284	18.760103	-0.051537	1.743403
279.903717	839.334262	18.765107	-0.051508	1.737024
279.901048	831.438410	18.770112	-0.051502	1.730605
279.693536	823.594043	18.775117	-0.051458	1.724178
279.859798	815.689487	18.780122	-0.051483	1.717725
279.800615	807.816928	18.785127	-0.051467	1.711246
279.610191	799.941066	18.790131	-0.051426	1.704722
279.631120	792.076806	18.795136	-0.051424	1.698210
279.566414	784.195460	18.800141	-0.051407	1.691648
279.550404	776.308635	18.805146	-0.051398	1.685061
279.589526	768.456328	18.810151	-0.051400	1.678486
279.415759	760.596792	18.815155	-0.051363	1.671849
279.261465	752.735056	18.820160	-0.051328	1.665188
279.176457	744.890560	18.825165	-0.051307	1.658523
279.148673	737.006864	18.830170	-0.051297	1.651806
279.140255	729.136813	18.835175	-0.051290	1.645075
278.885696	721.328560	18.840179	-0.051237	1.638337
278.960216	713.407382	18.845184	-0.051245	1.631518
278.846037	705.529192	18.850189	-0.051218	1.624681
278.686103	697.699602	18.855194	-0.051183	1.617852
278.828636	689.822760	18.860199	-0.051204	1.610995
278.812640	681.962034	18.865203	-0.051196	1.604100
278.511880	674.172662	18.870208	-0.051135	1.597199
278.804093	666.255792	18.875213	-0.051184	1.590238
278.623828	658.426481	18.880218	-0.051145	1.583258
278.347985	650.643914	18.885223	-0.051088	1.576274
278.268494	642.787728	18.890227	-0.051068	1.569222
278.458115	634.915772	18.895232	-0.051098	1.562162
278.226240	627.123534	18.900237	-0.051049	1.555081
278.043821	619.273240	18.905242	-0.051010	1.547923
278.167308	611.418993	18.910247	-0.051027	1.540772
277.982190	603.606590	18.915251	-0.050987	1.533581
278.002278	595.758047	18.920256	-0.050986	1.526353
278.065254	587.931518	18.925261	-0.050992	1.519117
278.072454	580.090091	18.930266	-0.050988	1.511825
277.945244	572.282330	18.935271	-0.050959	1.504508
277.837950	564.480341	18.940275	-0.050934	1.497164
277.843048	556.655725	18.945280	-0.050929	1.489780
277.846413	548.839553	18.950285	-0.050924	1.482367
277.702719	541.048255	18.955290	-0.050892	1.474917
277.720744	533.190237	18.960295	-0.050890	1.467390
277.517858	525.401742	18.965299	-0.050847	1.459857
277.547404	517.598164	18.970304	-0.050847	1.452307
277.325625	509.817999	18.975309	-0.050800	1.444701
277.286075	502.032713	18.980314	-0.050788	1.437078
277.157877	494.244888	18.985319	-0.050759	1.429398
277.127189	486.442558	18.990323	-0.050747	1.421677
277.206053	478.650167	18.995328	-0.050757	1.413943
276.957182	470.886095	19.000333	-0.050705	1.406140
276.860290	463.128672	19.005338	-0.050682	1.398326
277.066624	455.301940	19.010343	-0.050715	1.390448
277.094700	447.506829	19.015347	-0.050715	1.382527
276.767745	439.791218	19.020352	-0.050648	1.374582
276.602863	432.027857	19.025357	-0.050612	1.366569
276.522670	424.274790	19.030362	-0.050592	1.358534
276.409504	416.526405	19.035367	-0.050566	1.350451
276.391986	408.748546	19.040371	-0.050557	1.342304
276.258822	401.024865	19.045376	-0.050527	1.334144
276.212467	393.260082	19.050381	-0.050513	1.325906
276.023073	385.553951	19.055386	-0.050472	1.317654
276.135556	377.684761	19.060391	-0.050488	1.309228
276.114359	369.917746	19.065395	-0.050478	1.300835
276.147163	362.193650	19.070400	-0.050479	1.292443
275.966032	354.499507	19.075405	-0.050440	1.283990
275.678794	346.828746	19.080410	-0.050381	1.275487
275.723227	339.098079	19.085415	-0.050384	1.266922
275.602799	331.403539	19.090419	-0.050357	1.258309
275.579363	323.699757	19.095424	-0.050347	1.249644
275.418991	316.025031	19.100429	-0.050312	1.240925
275.302775	308.339581	19.105434	-0.050285	1.232140
275.415449	300.618068	19.110439	-0.050301	1.223296
275.444562	292.923173	19.115443	-0.050301	1.214402
275.011663	285.311701	19.120448	-0.050215	1.205447
274.860564	277.675056	19.125453	-0.050181	1.196453
274.789460	269.989932	19.130458	-0.050163	1.187349
274.803991	262.336964	19.135463	-0.050160	1.178230
274.849775	254.661786	19.140467	-0.050163	1.169020
274.811455	247.033991	19.145472	-0.050151	1.159777
274.611052	239.404053	19.150477	-0.050109	1.150423
274.462542	231.768687	19.155482	-0.050076	1.140997
274.393445	224.161308	19.160487	-0.050057	1.131543
274.133347	216.573432	19.165491	-0.050004	1.121994
274.219382	208.955502	19.170496	-0.050015	1.112399
274.266780	201.335682	19.175501	-0.050018	1.102710
274.302923	193.735671	19.180506	-0.050020	1.092959
274.179506	186.183731	19.185511	-0.049991	1.083146
273.962433	178.646198	19.190515	-0.049946	1.073241
274.124756	171.043611	19.195520	-0.049971	1.063245
273.857070	163.542572	19.200525	-0.049916	1.053190
273.577311	156.040489	19.205530	-0.049858	1.043033
273.476727	148.529791	19.210535	-0.049835	1.032808
273.393980	141.004902	19.215539	-0.049814	1.022465
273.418074	133.493842	19.220544	-0.049813	1.012061
273.287783	126.020033	19.225549	-0.049784	1.001563
273.001173	118.566452	19.230554	-0.049725	0.990945
272.985481	111.075310	19.235559	-0.049717	0.980225
272.656548	103.662908	19.240563	-0.049651	0.969421
272.740714	96.204767	19.245568	-0.049661	0.958535
272.650682	88.785314	19.250573	-0.049639	0.947536
272.442815	81.401880	19.255578	-0.049596	0.936430
272.450022	73.999952	19.260583	-0.049592	0.925221
272.420508	66.625693	19.265587	-0.049581	0.913906
272.137302	59.531956	19.270592	-0.049524	0.902819