Fri Mar 12 11:20:47 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
1.058117	-0.024752	0.000000	-0.000025	0.717385
0.775760	0.023835	0.005005	0.000028	0.717381
0.974945	-0.012681	0.010010	-0.000009	0.717378
1.038877	-0.019777	0.015014	-0.000020	0.717386
0.988354	-0.014655	0.020019	-0.000011	0.717378
0.871114	0.010006	0.025024	0.000011	0.717385
0.628981	0.050600	0.030029	0.000057	0.717380
0.946093	-0.006092	0.035034	-0.000002	0.717379
0.949619	-0.004244	0.040038	-0.000003	0.717383
0.864989	0.008413	0.045043	0.000013	0.717378
0.832839	0.017011	0.050048	0.000020	0.717383
0.943682	-0.003335	0.055053	-0.000001	0.717382
0.970754	-0.009943	0.060058	-0.000006	0.717378
1.067640	-0.021883	0.065062	-0.000023	0.717388
0.955263	-0.009058	0.070067	-0.000002	0.717373
0.798857	-0.127660	0.075072	0.000027	0.717083
0.933817	-0.150211	0.080077	0.000002	0.717085
0.923272	-0.150354	0.085082	0.000004	0.717081
0.990901	-0.158506	0.090086	-0.000008	0.717088
0.913610	-0.148772	0.095091	0.000007	0.717080
0.987590	-0.160776	0.100096	-0.000007	0.717082
1.142300	-0.241276	0.105101	-0.000035	0.716976
1.003502	-0.330604	0.110106	-0.000009	0.716750
1.231188	-0.365612	0.115110	-0.000051	0.716761
1.211959	-0.367717	0.120115	-0.000047	0.716749
1.178221	-0.357380	0.125120	-0.000041	0.716758
1.031963	-0.420708	0.130125	-0.000013	0.716580
0.943668	-0.473374	0.135130	0.000003	0.716444
1.107785	-0.497219	0.140134	-0.000027	0.716454
0.871869	-0.459933	0.145139	0.000017	0.716445
1.222926	-0.578910	0.150144	-0.000048	0.716332
1.210029	-0.674450	0.155149	-0.000045	0.716138
0.784255	-0.602080	0.160154	0.000034	0.716131
1.018841	-0.639663	0.165158	-0.000009	0.716139
0.907215	-0.709713	0.170163	0.000012	0.715960
0.788497	-0.724844	0.175168	0.000034	0.715888
0.945051	-0.751994	0.180173	0.000005	0.715889
0.853378	-0.778910	0.185178	0.000023	0.715803
0.910169	-0.914660	0.190182	0.000012	0.715553
0.894993	-0.915744	0.195187	0.000015	0.715545
0.969605	-0.941956	0.200192	0.000002	0.715519
0.979887	-1.087037	0.205197	0.000000	0.715234
0.675915	-1.035924	0.210202	0.000057	0.715228
0.788791	-1.077483	0.215206	0.000036	0.715185
0.700475	-1.203673	0.220211	0.000053	0.714903
0.785443	-1.216342	0.225216	0.000037	0.714907
0.752351	-1.263345	0.230221	0.000044	0.714802
0.627368	-1.339256	0.235226	0.000067	0.714606
0.825933	-1.368823	0.240230	0.000031	0.714618
0.599054	-1.450173	0.245235	0.000073	0.714375
0.558040	-1.490460	0.250240	0.000081	0.714280
0.786805	-1.555664	0.255245	0.000039	0.714231
0.767211	-1.685738	0.260250	0.000043	0.713965
0.945483	-1.712756	0.265254	0.000010	0.713974
0.757389	-1.815981	0.270259	0.000045	0.713702
0.583731	-1.811745	0.275264	0.000078	0.713649
0.471120	-1.862383	0.280269	0.000099	0.713508
0.356937	-1.917515	0.285274	0.000121	0.713357
0.202249	-1.917037	0.290278	0.000150	0.713303
0.080163	-2.038479	0.295283	0.000173	0.713017
0.096167	-2.038554	0.300288	0.000170	0.713022
0.170914	-2.190620	0.305293	0.000156	0.712746
-0.049224	-2.171124	0.310298	0.000198	0.712706
-0.200245	-2.246884	0.315302	0.000226	0.712501
-1.374520	-2.096637	0.320307	0.000445	0.712383
-1.389983	-2.114775	0.325312	0.000448	0.712341
-1.874991	-2.153958	0.330317	0.000538	0.712091
-2.267428	-2.086977	0.335322	0.000612	0.712084
-2.244533	-2.138181	0.340326	0.000608	0.711990
-3.231390	-2.079847	0.345331	0.000792	0.711755
-2.956029	-2.125868	0.350336	0.000741	0.711761
-3.369437	-2.070611	0.355341	0.000818	0.711724
-4.035283	-2.088917	0.360346	0.000942	0.711450
-3.735286	-2.140661	0.365350	0.000886	0.711453
-4.644539	-1.981697	0.370355	0.001056	0.711446
-4.480764	-2.091136	0.375360	0.001026	0.711286
-4.805310	-2.107125	0.380365	0.001086	0.711138
-5.159237	-2.047154	0.385370	0.001152	0.711132
-5.036640	-2.064002	0.390374	0.001130	0.711141
-5.146274	-2.106110	0.395379	0.001151	0.711018
-5.870935	-2.051745	0.400384	0.001286	0.710868
-5.590887	-2.099898	0.405389	0.001234	0.710871
-5.834849	-2.061006	0.410394	0.001279	0.710861
-5.445428	-2.169583	0.415398	0.001207	0.710783
-6.683712	-2.078100	0.420403	0.001438	0.710524
-6.885414	-2.038763	0.425408	0.001476	0.710531
-6.640603	-2.081303	0.430413	0.001430	0.710532
-6.668377	-2.080308	0.435418	0.001436	0.710524
-6.550999	-2.176020	0.440422	0.001414	0.710374
-7.860878	-2.025256	0.445427	0.001658	0.710208
-7.642204	-2.061069	0.450432	0.001618	0.710214
-7.704128	-2.048831	0.455437	0.001630	0.710216
-7.949735	-2.009521	0.460442	0.001676	0.710207
-7.360904	-2.147585	0.465446	0.001566	0.710140
-8.627410	-2.049534	0.470451	0.001802	0.709885
-8.721462	-2.032937	0.475456	0.001820	0.709884
-8.368986	-2.093027	0.480461	0.001755	0.709889
-8.506545	-2.069613	0.485466	0.001781	0.709886
-8.559006	-2.057030	0.490470	0.001791	0.709892
-8.711318	-2.090675	0.495475	0.001819	0.709770
-9.329220	-2.069978	0.500480	0.001934	0.709591
-9.007102	-2.126221	0.505485	0.001875	0.709593
-9.426415	-2.054739	0.510490	0.001953	0.709586
-9.238174	-2.082206	0.515494	0.001918	0.709598
-9.396747	-2.057894	0.520499	0.001948	0.709589
-9.981936	-2.057943	0.525504	0.002057	0.709380
-10.273061	-2.064032	0.530509	0.002112	0.709264
-10.055156	-2.105605	0.535514	0.002071	0.709258
-10.338918	-2.051139	0.540518	0.002124	0.709265
-10.334413	-2.055732	0.545523	0.002124	0.709257
-9.928341	-2.126550	0.550528	0.002048	0.709260
-9.982424	-2.191644	0.555533	0.002059	0.709110
-11.699491	-1.967626	0.560538	0.002379	0.708945
-10.967608	-2.091407	0.565542	0.002243	0.708958
-11.021955	-2.087342	0.570547	0.002253	0.708946
-11.312995	-2.033334	0.575552	0.002307	0.708950
-10.906814	-2.104524	0.580557	0.002232	0.708952
-10.966989	-2.105425	0.585562	0.002243	0.708928
-11.710846	-2.117657	0.590566	0.002382	0.708638
-11.881984	-2.089461	0.595571	0.002414	0.708633
-12.053942	-2.055547	0.600576	0.002446	0.708639
-11.663046	-2.124366	0.605581	0.002374	0.708640
-12.442510	-1.989541	0.610586	0.002519	0.708631
-12.280876	-2.012277	0.615590	0.002489	0.708643
-12.069497	-2.099795	0.620595	0.002450	0.708543
-13.374347	-1.964436	0.625600	0.002693	0.708348
-12.942885	-2.040253	0.630605	0.002613	0.708349
-13.037672	-2.025858	0.635610	0.002631	0.708344
-12.786391	-2.065549	0.640614	0.002585	0.708354
-12.900822	-2.049757	0.645619	0.002606	0.708344
-12.639545	-2.094345	0.650624	0.002558	0.708347
-12.558741	-2.193309	0.655629	0.002543	0.708178
-14.244731	-1.978552	0.660634	0.002857	0.708005
-13.677247	-2.075734	0.665638	0.002752	0.708013
-13.672789	-2.078015	0.670643	0.002751	0.708009
-14.091572	-2.003612	0.675648	0.002829	0.708008
-13.822172	-2.050585	0.680653	0.002780	0.708010
-13.888447	-2.041504	0.685658	0.002792	0.708004
-13.912545	-2.114332	0.690662	0.002797	0.707849
-15.108911	-1.979753	0.695667	0.003020	0.707691
-14.771799	-2.039535	0.700672	0.002957	0.707691
-14.412123	-2.101472	0.705677	0.002891	0.707695
-15.098693	-1.982839	0.710682	0.003019	0.707687
-14.679492	-2.053479	0.715686	0.002941	0.707695
-14.675474	-2.056653	0.720691	0.002940	0.707689
-15.037308	-2.032945	0.725696	0.003008	0.707607
-15.465851	-2.075064	0.730701	0.003088	0.707369
-15.301243	-2.108183	0.735706	0.003058	0.707361
-15.503659	-2.066237	0.740710	0.003095	0.707372
-15.717270	-2.030852	0.745715	0.003135	0.707366
-15.494853	-2.068442	0.750720	0.003094	0.707370
-15.401352	-2.081770	0.755725	0.003077	0.707376
-15.821950	-2.086689	0.760730	0.003156	0.707215
-16.645153	-2.007540	0.765734	0.003309	0.707079
-16.419551	-2.051453	0.770739	0.003267	0.707071
-16.554925	-2.026046	0.775744	0.003293	0.707073
-16.400237	-2.050710	0.780749	0.003264	0.707079
-16.461409	-2.044866	0.785754	0.003276	0.707068
-16.195008	-2.087110	0.790758	0.003227	0.707078
-16.294854	-2.158262	0.795763	0.003245	0.706899
-17.490871	-2.022611	0.800768	0.003468	0.706743
-17.011109	-2.105765	0.805773	0.003379	0.706747
-17.625512	-1.999323	0.810778	0.003494	0.706741
-17.505681	-2.016570	0.815782	0.003472	0.706748
-16.982382	-2.111332	0.820787	0.003375	0.706745
-17.323110	-2.050253	0.825792	0.003438	0.706745
-17.584063	-2.107017	0.830797	0.003487	0.706537
-18.325187	-2.028170	0.835802	0.003625	0.706430
-17.971993	-2.084765	0.840806	0.003560	0.706442
-18.335696	-2.023784	0.845811	0.003628	0.706434
-18.376621	-2.013776	0.850816	0.003636	0.706439
-18.010544	-2.077018	0.855821	0.003568	0.706443
-18.317639	-2.027487	0.860826	0.003625	0.706432
-18.160896	-2.156213	0.865830	0.003596	0.706229
-18.922734	-2.073336	0.870835	0.003738	0.706122
-19.025623	-2.055389	0.875840	0.003758	0.706121
-19.190743	-2.023282	0.880845	0.003789	0.706125
-19.271981	-2.012262	0.885850	0.003804	0.706118
-18.726728	-2.105194	0.890854	0.003703	0.706126
-18.906629	-2.074334	0.895859	0.003736	0.706123
-19.649199	-2.066997	0.900864	0.003875	0.705871
-19.618192	-2.076838	0.905869	0.003869	0.705862
-20.226066	-1.973023	0.910874	0.003983	0.705853
-19.902418	-2.026765	0.915878	0.003923	0.705860
-19.787680	-2.051183	0.920883	0.003902	0.705852
-19.812224	-2.045882	0.925888	0.003906	0.705853
-19.600739	-2.100353	0.930893	0.003867	0.705819
-20.607208	-2.071087	0.935898	0.004055	0.705516
-20.392984	-2.106101	0.940902	0.004015	0.705522
-20.905965	-2.016250	0.945907	0.004111	0.705519
-20.853753	-2.025447	0.950912	0.004102	0.705518
-20.447102	-2.096006	0.955917	0.004026	0.705522
-20.954495	-2.011107	0.960922	0.004121	0.705510
-20.669974	-2.108958	0.965926	0.004068	0.705415
-21.629214	-2.043395	0.970931	0.004247	0.705202
-21.430829	-2.077643	0.975936	0.004210	0.705204
-21.610715	-2.042788	0.980941	0.004244	0.705209
-21.744338	-2.022927	0.985946	0.004269	0.705201
-21.247783	-2.107035	0.990950	0.004177	0.705209
-21.495090	-2.064697	0.995955	0.004223	0.705205
-21.797737	-2.100493	1.000960	0.004280	0.705024
-22.433399	-2.056046	1.005965	0.004398	0.704885
-22.701490	-2.012520	1.010970	0.004448	0.704876
-22.729866	-2.003204	1.015974	0.004454	0.704884
-22.542262	-2.039523	1.020979	0.004419	0.704878
-22.494915	-2.049132	1.025984	0.004411	0.704875
-22.586805	-2.028919	1.030989	0.004428	0.704882
-22.790416	-2.023239	1.035994	0.004466	0.704820
-23.021013	-2.097663	1.040998	0.004509	0.704587
-23.053537	-2.095627	1.046003	0.004516	0.704579
-23.656217	-1.986289	1.051008	0.004628	0.704582
-23.130652	-2.077436	1.056013	0.004531	0.704587
-23.462785	-2.023226	1.061018	0.004593	0.704576
-23.553268	-2.003652	1.066022	0.004610	0.704583
-23.240435	-2.119696	1.071027	0.004552	0.704461
-24.220925	-2.050454	1.076032	0.004734	0.704248
-24.208148	-2.047433	1.081037	0.004732	0.704258
-24.485065	-2.001708	1.086042	0.004784	0.704250
-24.255613	-2.039640	1.091046	0.004742	0.704256
-24.313201	-2.032050	1.096051	0.004753	0.704250
-24.770957	-1.949438	1.101056	0.004838	0.704251
-24.381057	-2.028209	1.106061	0.004766	0.704232
-25.029537	-2.056859	1.111066	0.004887	0.703941
-25.206195	-2.021654	1.116070	0.004920	0.703948
-25.388071	-1.991670	1.121075	0.004954	0.703942
-24.973783	-2.065383	1.126080	0.004877	0.703942
-25.023258	-2.053433	1.131085	0.004886	0.703948
-25.465612	-1.976469	1.136090	0.004969	0.703944
-24.704550	-2.131317	1.141094	0.004828	0.703905
-25.674853	-2.094627	1.146099	0.005009	0.703629
-25.956069	-2.048091	1.151104	0.005061	0.703622
-26.042422	-2.027904	1.156109	0.005077	0.703631
-25.792889	-2.075996	1.161114	0.005031	0.703623
-25.897598	-2.054392	1.166118	0.005051	0.703629
-26.082806	-2.021183	1.171123	0.005086	0.703628
-26.035973	-2.090763	1.176128	0.005077	0.703504
-26.763016	-2.043311	1.181133	0.005213	0.703338
-27.022341	-1.999555	1.186138	0.005261	0.703333
-26.683393	-2.057054	1.191142	0.005198	0.703338
-26.778796	-2.040745	1.196147	0.005216	0.703336
-27.143363	-1.976252	1.201152	0.005285	0.703335
-26.584704	-2.071765	1.206157	0.005181	0.703343
-26.773155	-2.134777	1.211162	0.005216	0.703147
-27.977561	-1.990997	1.216166	0.005441	0.703003
-27.772140	-2.028633	1.221171	0.005403	0.703001
-27.552430	-2.068392	1.226176	0.005362	0.702999
-27.662258	-2.045955	1.231181	0.005383	0.703004
-28.173296	-1.959093	1.236186	0.005478	0.702995
-27.874512	-2.007618	1.241190	0.005423	0.703005
-27.567741	-2.131795	1.246195	0.005366	0.702864
-28.803916	-2.000201	1.251200	0.005596	0.702684
-28.386003	-2.070781	1.256205	0.005519	0.702691
-28.798745	-2.002639	1.261210	0.005596	0.702680
-28.793290	-1.998788	1.266214	0.005595	0.702689
-28.490653	-2.052677	1.271219	0.005539	0.702689
-28.530681	-2.047205	1.276224	0.005546	0.702685
-28.528854	-2.134394	1.281229	0.005546	0.702509
-29.860888	-1.970290	1.286234	0.005795	0.702360
-29.528679	-2.025013	1.291238	0.005733	0.702369
-29.345775	-2.060989	1.296243	0.005699	0.702362
-29.642532	-2.007424	1.301248	0.005755	0.702362
-29.486330	-2.031265	1.306253	0.005726	0.702370
-29.438317	-2.044039	1.311258	0.005717	0.702361
-29.575765	-2.089523	1.316262	0.005743	0.702219
-30.563641	-1.987173	1.321267	0.005927	0.702069
-30.300757	-2.036214	1.326272	0.005878	0.702065
-30.283179	-2.036150	1.331277	0.005875	0.702071
-30.600423	-1.983407	1.336282	0.005935	0.702062
-30.120852	-2.063444	1.341286	0.005846	0.702073
-30.277293	-2.037406	1.346291	0.005875	0.702069
-30.730790	-2.055246	1.351296	0.005960	0.701869
-31.330413	-2.011747	1.356301	0.006072	0.701740
-31.074810	-2.061341	1.361306	0.006024	0.701731
-31.072441	-2.056368	1.366310	0.006024	0.701742
-31.601620	-1.962475	1.371315	0.006123	0.701740
-31.431415	-1.994758	1.376320	0.006091	0.701736
-31.002543	-2.066685	1.381325	0.006012	0.701745
-31.270306	-2.103559	1.386330	0.006062	0.701573
-32.057129	-2.032240	1.391334	0.006209	0.701433
-31.810677	-2.076769	1.396339	0.006163	0.701431
-32.148285	-2.018268	1.401344	0.006226	0.701427
-32.133842	-2.016877	1.406349	0.006224	0.701435
-31.982809	-2.048016	1.411354	0.006196	0.701426
-32.061203	-2.031728	1.416358	0.006210	0.701430
-32.509935	-2.069243	1.421363	0.006294	0.701192
-33.215501	-1.981043	1.426368	0.006426	0.701115
-32.692242	-2.069962	1.431373	0.006329	0.701124
-32.911490	-2.037421	1.436378	0.006370	0.701110
-33.234674	-1.976365	1.441382	0.006430	0.701116
-33.009107	-2.016747	1.446387	0.006388	0.701115
-33.067033	-2.008155	1.451392	0.006399	0.701111
-33.007603	-2.097090	1.456397	0.006389	0.700952
-33.699046	-2.016631	1.461402	0.006518	0.700865
-33.655477	-2.022094	1.466406	0.006510	0.700869
-33.655046	-2.022791	1.471411	0.006510	0.700868
-33.608497	-2.031828	1.476416	0.006501	0.700866
-33.240914	-2.093144	1.481421	0.006433	0.700874
-33.715705	-2.070341	1.486426	0.006522	0.700748
-34.910677	-1.964801	1.491430	0.006745	0.700529
-34.350299	-2.064044	1.496435	0.006641	0.700530
-34.745341	-1.994717	1.501440	0.006714	0.700528
-34.637632	-2.009308	1.506445	0.006694	0.700537
-34.500002	-2.037937	1.511450	0.006669	0.700528
-34.329419	-2.065011	1.516454	0.006638	0.700534
-34.602141	-2.113854	1.521459	0.006689	0.700336
-35.677914	-1.984554	1.526464	0.006889	0.700209
-35.249631	-2.056779	1.531469	0.006810	0.700217
-35.597877	-1.998681	1.536474	0.006875	0.700208
-35.759707	-1.967286	1.541478	0.006905	0.700213
-35.395197	-2.029946	1.546483	0.006837	0.700217
-35.626273	-1.990089	1.551488	0.006881	0.700214
-35.837164	-2.043446	1.556493	0.006920	0.700029
-36.707507	-1.957903	1.561498	0.007082	0.699887
-36.092403	-2.064025	1.566502	0.006968	0.699894
-36.243945	-2.039696	1.571507	0.006997	0.699888
-36.631000	-1.971366	1.576512	0.007069	0.699886
-36.069212	-2.067172	1.581517	0.006965	0.699895
-36.378001	-2.017339	1.586522	0.007022	0.699883
-36.621859	-2.060349	1.591526	0.007068	0.699707
-37.209322	-2.009801	1.596531	0.007178	0.699597
-37.297840	-1.995863	1.601536	0.007194	0.699593
-37.206872	-2.008399	1.606541	0.007178	0.699600
-37.146763	-2.022045	1.611546	0.007167	0.699593
-36.990443	-2.049619	1.616550	0.007138	0.699593
-37.096167	-2.030114	1.621555	0.007158	0.699594
-37.826938	-2.038289	1.626560	0.007294	0.699313
-37.861886	-2.054696	1.631565	0.007301	0.699266
-38.188118	-2.000629	1.636570	0.007362	0.699257
-38.072824	-2.017314	1.641574	0.007340	0.699265
-38.106089	-2.011193	1.646579	0.007347	0.699265
-38.226097	-1.991676	1.651584	0.007369	0.699260
-38.095348	-2.011540	1.656589	0.007345	0.699267
-38.108036	-2.133806	1.661594	0.007348	0.699014
-38.787626	-2.041954	1.666598	0.007475	0.698953
-38.872219	-2.026716	1.671603	0.007491	0.698953
-39.211846	-1.968606	1.676608	0.007554	0.698948
-38.718699	-2.050877	1.681613	0.007463	0.698959
-39.012342	-2.001774	1.686618	0.007518	0.698952
-39.125066	-1.992006	1.691622	0.007539	0.698930
-39.615925	-2.049237	1.696627	0.007630	0.698636
-39.861709	-2.006249	1.701632	0.007676	0.698633
-39.942386	-1.986987	1.706637	0.007692	0.698643
-39.931841	-1.993978	1.711642	0.007690	0.698632
-39.777011	-2.018985	1.716646	0.007661	0.698637
-39.886541	-1.999223	1.721651	0.007682	0.698637
-40.029467	-1.975616	1.726656	0.007709	0.698633
-40.023739	-2.093948	1.731661	0.007708	0.698394
-40.781307	-1.983703	1.736666	0.007849	0.698343
-40.965194	-1.947110	1.741670	0.007884	0.698350
-40.436020	-2.040266	1.746675	0.007785	0.698352
-40.700563	-1.996848	1.751680	0.007835	0.698344
-40.388253	-2.048370	1.756685	0.007777	0.698352
-40.625969	-2.034910	1.761690	0.007822	0.698292
-41.113727	-2.085725	1.766694	0.007913	0.698012
-40.800983	-2.141394	1.771699	0.007855	0.698011
-41.910345	-1.947904	1.776704	0.008061	0.698002
-41.472310	-2.019975	1.781709	0.007980	0.698014
-41.338303	-2.048022	1.786714	0.007955	0.698005
-41.459209	-2.022931	1.791718	0.007978	0.698012
-41.531656	-2.111490	1.796723	0.007992	0.697805
-42.542106	-1.987475	1.801728	0.008180	0.697690
-42.343165	-2.017786	1.806733	0.008143	0.697700
-42.586966	-1.977984	1.811738	0.008189	0.697692
-42.297433	-2.028479	1.816742	0.008135	0.697694
-41.987023	-2.083733	1.821747	0.008078	0.697694
-42.357711	-2.020839	1.826752	0.008147	0.697687
-42.539437	-2.113311	1.831757	0.008181	0.697432
-43.127789	-2.038991	1.836762	0.008291	0.697369
-43.184332	-2.026800	1.841766	0.008302	0.697373
-43.152123	-2.031284	1.846771	0.008296	0.697375
-43.299092	-2.009211	1.851776	0.008324	0.697366
-43.081941	-2.042007	1.856781	0.008283	0.697378
-43.190652	-2.037449	1.861786	0.008304	0.697347
-43.743267	-2.070174	1.866790	0.008407	0.697079
-43.829887	-2.054037	1.871795	0.008423	0.697080
-44.467962	-1.942753	1.876800	0.008542	0.697074
-43.979298	-2.024212	1.881805	0.008452	0.697086
-43.901599	-2.042671	1.886810	0.008437	0.697076
-44.180762	-1.989585	1.891814	0.008490	0.697082
-43.934870	-2.069489	1.896819	0.008444	0.697008
-44.773463	-2.047230	1.901824	0.008600	0.696748
-44.384965	-2.111018	1.906829	0.008528	0.696759
-44.947266	-2.015008	1.911834	0.008633	0.696750
-44.924032	-2.016972	1.916838	0.008629	0.696754
-44.568349	-2.080305	1.921843	0.008563	0.696753
-45.137861	-1.982473	1.926848	0.008669	0.696745
-45.212086	-2.055095	1.931853	0.008684	0.696570
-45.745206	-2.025405	1.936858	0.008783	0.696436
-45.852998	-2.002697	1.941862	0.008803	0.696442
-45.706537	-2.027754	1.946867	0.008776	0.696444
-45.809205	-2.013078	1.951872	0.008796	0.696436
-45.394567	-2.082796	1.956877	0.008719	0.696444
-45.838327	-2.007237	1.961882	0.008802	0.696437
-46.194644	-2.045988	1.966886	0.008868	0.696227
-46.353555	-2.066415	1.971891	0.008898	0.696128
-46.503388	-2.041831	1.976896	0.008926	0.696123
-46.448139	-2.047826	1.981901	0.008916	0.696130
-46.608362	-2.022498	1.986906	0.008946	0.696123
-46.303275	-2.074552	1.991910	0.008890	0.696127
-46.413787	-2.066124	1.996915	0.008910	0.696104
-47.162034	-2.044048	2.001920	0.009050	0.695876
-47.463246	-1.992734	2.011917	0.009106	0.695870
-47.128208	-2.052544	2.021914	0.009045	0.695869
-47.366265	-2.007557	2.031910	0.009089	0.695873
-47.202568	-2.037109	2.041907	0.009059	0.695872
-47.247589	-2.028203	2.051904	0.009068	0.695873
-47.439367	-1.995721	2.061901	0.009104	0.695868
-47.427567	-1.996875	2.071898	0.009103	0.695869
-47.265903	-2.024800	2.081894	0.009073	0.695870
-47.293809	-2.018986	2.091891	0.009079	0.695871
-47.371775	-2.005237	2.101888	0.009094	0.695870
-47.425931	-1.996271	2.111885	0.009104	0.695867
-47.188860	-2.036117	2.121882	0.009061	0.695871
-47.336230	-2.008762	2.131878	0.009089	0.695873
-46.715921	-2.027224	2.141875	0.008974	0.696060
-46.471598	-2.038683	2.151872	0.008929	0.696124
-46.576855	-2.020181	2.161869	0.008949	0.696123
-46.522596	-2.029713	2.171866	0.008939	0.696122
-46.551886	-2.016451	2.181862	0.008945	0.696138
-45.618485	-2.033408	2.191859	0.008772	0.696442
-45.734597	-2.012358	2.201856	0.008794	0.696442
-45.813626	-2.000029	2.211853	0.008809	0.696437
-45.732036	-2.008804	2.221850	0.008794	0.696448
-45.306603	-1.935692	2.231846	0.008715	0.696751
-44.777968	-2.029074	2.241843	0.008617	0.696752
-45.081037	-1.975557	2.251840	0.008674	0.696750
-44.740033	-1.959868	2.261837	0.008611	0.696905
-43.947159	-2.015366	2.271834	0.008464	0.697079
-44.077746	-1.992041	2.281830	0.008489	0.697078
-43.809247	-2.038522	2.291827	0.008439	0.697080
-43.479073	-1.988329	2.301824	0.008378	0.697302
-43.331286	-1.980281	2.311821	0.008351	0.697371
-43.252586	-1.993405	2.321818	0.008337	0.697372
-43.068341	-1.978464	2.331814	0.008303	0.697468
-42.107108	-2.036851	2.341811	0.008125	0.697697
-42.142057	-2.031238	2.351808	0.008132	0.697695
-42.235947	-2.014921	2.361805	0.008150	0.697693
-41.872976	-1.983878	2.371802	0.008083	0.697887
-41.210735	-2.041865	2.381798	0.007960	0.698009
-41.414769	-2.004252	2.391795	0.007998	0.698010
-41.225155	-2.039423	2.401792	0.007963	0.698007
-40.518415	-2.008174	2.411789	0.007832	0.698326
-40.471547	-2.006320	2.421786	0.007824	0.698346
-40.197153	-2.054230	2.431782	0.007773	0.698347
-40.213087	-2.021691	2.441779	0.007777	0.698406
-39.644431	-2.009506	2.451776	0.007671	0.698636
-39.579301	-2.022014	2.461773	0.007660	0.698634
-39.648232	-2.007422	2.471770	0.007673	0.698637
-39.139395	-1.982951	2.481766	0.007579	0.698871
-38.718918	-2.017224	2.491763	0.007501	0.698953
-38.757749	-2.011575	2.501760	0.007509	0.698949
-38.563916	-2.004537	2.511757	0.007473	0.699033
-38.203541	-1.956596	2.521754	0.007406	0.699260
-37.817938	-2.023182	2.531750	0.007335	0.699263
-37.734674	-2.037924	2.541747	0.007320	0.699263
-37.227766	-1.975736	2.551744	0.007226	0.699571
-36.948914	-2.015581	2.561741	0.007175	0.699591
-36.830309	-2.036088	2.571738	0.007153	0.699591
-36.730687	-2.006585	2.581734	0.007135	0.699686
-36.124652	-2.012780	2.591731	0.007023	0.699892
-36.032895	-2.029461	2.601728	0.007006	0.699890
-36.230782	-1.994294	2.611725	0.007043	0.699889
-35.795963	-1.927196	2.621722	0.006963	0.700182
-35.184918	-2.019529	2.631718	0.006850	0.700214
-35.202791	-2.015580	2.641715	0.006853	0.700215
-34.832137	-2.004112	2.651712	0.006785	0.700371
-34.251084	-2.028142	2.661709	0.006677	0.700532
-34.481718	-1.988488	2.671706	0.006721	0.700528
-34.246536	-2.028239	2.681702	0.006677	0.700532
-33.736492	-1.964616	2.691699	0.006583	0.700844
-33.317660	-2.025275	2.701696	0.006505	0.700871
-33.370455	-2.017297	2.711693	0.006516	0.700868
-33.341292	-1.985901	2.721690	0.006511	0.700941
-32.580161	-2.033368	2.731686	0.006369	0.701119
-32.705345	-2.009897	2.741683	0.006393	0.701120
-32.799334	-1.993416	2.751680	0.006411	0.701119
-32.132395	-1.958443	2.761677	0.006287	0.701429
-31.792310	-2.019444	2.771674	0.006225	0.701428
-31.662715	-2.039358	2.781670	0.006201	0.701433
-31.462597	-1.986988	2.791667	0.006164	0.701611
-31.131274	-1.982167	2.801664	0.006103	0.701739
-31.055673	-1.995310	2.811661	0.006089	0.701739
-31.082085	-1.940439	2.821658	0.006095	0.701839
-29.874860	-2.042710	2.831654	0.005870	0.702067
-30.145891	-1.993388	2.841651	0.005921	0.702068
-30.102467	-2.001567	2.851648	0.005914	0.702066
-29.452976	-1.987031	2.861645	0.005793	0.702329
-29.285218	-1.998360	2.871642	0.005762	0.702366
-28.987699	-2.050648	2.881638	0.005708	0.702366
-29.233722	-1.937317	2.891635	0.005754	0.702506
-28.045703	-2.058050	2.901632	0.005533	0.702689
-28.348074	-2.007241	2.911629	0.005590	0.702682
-28.219924	-2.028593	2.921626	0.005566	0.702684
-27.465274	-2.044482	2.931622	0.005426	0.702923
-27.345552	-2.027187	2.941619	0.005405	0.703000
-27.213868	-2.049246	2.951616	0.005381	0.703002
-27.244308	-2.043790	2.961613	0.005387	0.703001
-26.795629	-1.956874	2.971610	0.005304	0.703337
-26.383166	-2.030270	2.981606	0.005227	0.703336
-26.502275	-2.009277	2.991603	0.005250	0.703335
-26.236940	-1.964641	3.001600	0.005201	0.703520
-25.839014	-1.980647	3.011597	0.005127	0.703630
-25.814979	-1.985098	3.021594	0.005123	0.703628
-25.444499	-2.011889	3.031590	0.005055	0.703707
-24.890650	-1.990471	3.041587	0.004952	0.703948
-24.810020	-2.005207	3.051584	0.004938	0.703946
-25.044922	-1.964656	3.061581	0.004982	0.703943
-24.099952	-1.997072	3.071578	0.004806	0.704216
-23.908951	-2.012607	3.081574	0.004771	0.704253
-24.100353	-1.977022	3.091571	0.004807	0.704255
-23.710459	-1.978660	3.101568	0.004735	0.704391
-23.050361	-2.003014	3.111565	0.004613	0.704578
-22.757917	-2.052836	3.121562	0.004559	0.704582
-22.964272	-2.015090	3.131558	0.004598	0.704583
-22.715127	-1.951487	3.141555	0.004552	0.704799
-22.222066	-1.998817	3.151552	0.004461	0.704880
-22.511000	-1.946155	3.161549	0.004515	0.704881
-21.941683	-1.969042	3.171546	0.004409	0.705039
-21.397703	-1.981607	3.181542	0.004308	0.705208
-21.278133	-2.001577	3.191539	0.004287	0.705210
-21.486379	-1.953828	3.201536	0.004326	0.705230
-20.484044	-1.987691	3.211533	0.004140	0.705521
-20.477125	-1.989364	3.221530	0.004139	0.705519
-20.481597	-1.987220	3.231526	0.004140	0.705521
-20.197211	-1.950027	3.241523	0.004088	0.705697
-19.288868	-2.030723	3.251520	0.003919	0.705859
-19.689416	-1.960188	3.261517	0.003994	0.705856
-19.354122	-2.018223	3.271514	0.003932	0.705859
-18.904024	-1.982616	3.281510	0.003849	0.706091
-18.732550	-1.995976	3.291507	0.003817	0.706125
-18.727476	-1.996893	3.301504	0.003817	0.706124
-18.254103	-2.022470	3.311501	0.003729	0.706241
-17.636632	-2.031293	3.321498	0.003615	0.706444
-18.002067	-1.964687	3.331494	0.003683	0.706446
-17.788521	-2.004322	3.341491	0.003644	0.706442
-17.360491	-1.949700	3.351488	0.003565	0.706704
-17.150792	-1.965616	3.361485	0.003526	0.706746
-16.811436	-2.024642	3.371482	0.003464	0.706748
-16.714501	-1.963679	3.381478	0.003446	0.706904
-15.810087	-2.038495	3.391475	0.003278	0.707077
-16.203424	-1.966956	3.401472	0.003352	0.707079
-16.111151	-1.984002	3.411469	0.003335	0.707077
-15.278379	-1.989792	3.421466	0.003180	0.707362
-15.191644	-1.999463	3.431462	0.003165	0.707373
-14.773184	-2.071962	3.441459	0.003087	0.707376
-15.249550	-1.935227	3.451456	0.003176	0.707479
-13.974965	-2.053188	3.461453	0.002940	0.707697
-14.265471	-2.001033	3.471450	0.002994	0.707697
-13.936337	-2.058505	3.481446	0.002933	0.707699
-13.407099	-2.066533	3.491443	0.002835	0.707871
-12.899195	-2.086290	3.501440	0.002741	0.708012
-12.930230	-2.081436	3.511437	0.002748	0.708010
-12.908759	-2.084732	3.521434	0.002744	0.708010
-12.824914	-2.042615	3.531430	0.002729	0.708123
-11.942655	-2.086987	3.541427	0.002565	0.708348
-12.185089	-2.042856	3.551424	0.002611	0.708349
-12.084988	-2.060322	3.561421	0.002592	0.708349
-11.756626	-2.030082	3.571418	0.002532	0.708526
-11.263800	-2.061829	3.581414	0.002441	0.708638
-11.117919	-2.086439	3.591411	0.002414	0.708639
-11.163567	-2.078319	3.601408	0.002423	0.708639
-10.528286	-2.046143	3.611405	0.002305	0.708929
-10.370889	-2.061485	3.621402	0.002276	0.708953
-10.210595	-2.089405	3.631398	0.002247	0.708954
-10.137042	-2.055877	3.641395	0.002234	0.709046
-9.412873	-2.076714	3.651392	0.002099	0.709262
-9.383682	-2.081307	3.661389	0.002094	0.709262
-9.492641	-2.061747	3.671386	0.002115	0.709262
-8.875071	-2.068706	3.681382	0.002000	0.709467
-8.375474	-2.093762	3.691379	0.001908	0.709594
-8.560903	-2.060067	3.701376	0.001943	0.709594
-8.467097	-2.077426	3.711373	0.001926	0.709592
-8.010138	-2.019826	3.721370	0.001841	0.709869
-7.304053	-2.133402	3.731366	0.001710	0.709893
-7.697880	-2.064053	3.741363	0.001784	0.709890
-7.534022	-2.032870	3.751360	0.001754	0.710010
-6.599589	-2.095670	3.761357	0.001581	0.710217
-6.682189	-2.081279	3.771354	0.001596	0.710215
-6.758480	-2.065392	3.781350	0.001611	0.710219
-6.168616	-2.043748	3.791347	0.001502	0.710471
-5.702715	-2.094707	3.801344	0.001416	0.710534
-5.949579	-2.052413	3.811341	0.001462	0.710530
-5.859549	-2.025548	3.821338	0.001446	0.710615
-4.749037	-2.095042	3.831334	0.001239	0.710870
-4.986037	-2.052943	3.841331	0.001284	0.710869
-4.796918	-2.084469	3.851328	0.001249	0.710872
-4.472231	-2.060164	3.861325	0.001189	0.711035
-4.100948	-2.076649	3.871322	0.001121	0.711134
-4.119602	-2.070326	3.881318	0.001124	0.711139
-4.119808	-2.044653	3.891315	0.001125	0.711189
-2.983770	-2.112859	3.901312	0.000914	0.711456
-3.144324	-2.084933	3.911309	0.000944	0.711454
-3.185709	-2.075773	3.921306	0.000953	0.711456
-2.851660	-2.054083	3.931302	0.000891	0.711617
-2.276633	-2.082565	3.941299	0.000784	0.711764
-2.200990	-2.095826	3.951296	0.000771	0.711764
-2.186226	-2.098709	3.961293	0.000768	0.711762
-1.645007	-2.039667	3.971290	0.000668	0.712071
-1.466425	-2.060799	3.981286	0.000635	0.712092
-1.559273	-2.043448	3.991283	0.000653	0.712092
-1.411334	-1.986753	4.001280	0.000626	0.712257
-0.943624	-2.005614	4.011277	0.000539	0.712384
-0.946859	-2.003211	4.021274	0.000540	0.712387
-1.149047	-1.872007	4.031270	0.000578	0.712576
-0.941530	-1.840629	4.041267	0.000540	0.712711
-0.922490	-1.814245	4.051264	0.000537	0.712769
-0.634791	-1.738077	4.061261	0.000484	0.713022
-0.605949	-1.743234	4.071258	0.000479	0.713021
-0.597178	-1.584165	4.081254	0.000478	0.713340
-0.744272	-1.544657	4.091251	0.000506	0.713365
-0.673401	-1.413791	4.101248	0.000493	0.713650
-0.603455	-1.382366	4.111245	0.000480	0.713736
-0.418565	-1.299423	4.121242	0.000446	0.713966
-0.159030	-1.251335	4.131238	0.000398	0.714152
-0.291894	-1.160654	4.141235	0.000423	0.714284
-0.291605	-0.996836	4.151232	0.000424	0.714609
-0.228035	-0.923552	4.161229	0.000412	0.714776
-0.145141	-0.845618	4.171226	0.000397	0.714959
-0.101368	-0.715156	4.181222	0.000390	0.715233
-0.066356	-0.587022	4.191219	0.000383	0.715498
-0.069804	-0.463733	4.201216	0.000385	0.715741
0.109928	-0.376938	4.211213	0.000351	0.715975
-0.083257	-0.229788	4.221210	0.000388	0.716198
-0.063746	-0.091055	4.231206	0.000385	0.716478
-0.060987	0.056086	4.241203	0.000384	0.716770
0.000000	0.241588	4.251200	0.000373	0.717158
0.067460	0.834723	4.256205	0.000361	0.718354
0.186768	2.059999	4.261210	0.000338	0.720811
0.502977	3.844518	4.266214	0.000278	0.724425
0.780564	6.193754	4.271219	0.000225	0.729108
0.967232	9.064540	4.276224	0.000189	0.734737
1.501340	12.357070	4.281229	0.000087	0.741250
1.696070	16.152396	4.286234	0.000049	0.748545
2.135512	20.329528	4.291238	-0.000035	0.756567
2.488150	24.893992	4.296243	-0.000104	0.765195
2.978206	29.818871	4.301248	-0.000198	0.774432
3.434612	35.093299	4.306253	-0.000286	0.784182
3.779005	40.711093	4.311258	-0.000354	0.794389
4.487429	46.559982	4.316262	-0.000489	0.804988
4.777948	52.774709	4.321267	-0.000547	0.815957
5.396696	59.189376	4.326272	-0.000666	0.827223
5.828117	65.898812	4.331277	-0.000751	0.838779
6.013813	72.837615	4.336282	-0.000790	0.850489
6.526234	79.938631	4.341286	-0.000889	0.862401
7.091939	87.221060	4.346291	-0.000999	0.874460
10.342236	94.196734	4.351296	-0.001609	0.886620
14.440414	101.292043	4.356301	-0.002376	0.899036
14.892749	109.179011	4.361306	-0.002465	0.911518
15.474856	117.157884	4.366310	-0.002579	0.924007
15.935175	125.268482	4.371315	-0.002669	0.936496
17.193511	133.335246	4.376320	-0.002909	0.948963
18.210852	141.550028	4.381325	-0.003103	0.961424
19.346853	149.821114	4.386330	-0.003320	0.973838
20.239733	158.215137	4.391334	-0.003492	0.986210
21.204902	166.668680	4.396339	-0.003677	0.998531
21.675163	175.219128	4.401344	-0.003769	1.010716
22.899480	183.688293	4.406349	-0.004003	1.022825
23.323831	192.329745	4.411354	-0.004087	1.034837
24.463504	200.863524	4.416358	-0.004305	1.046733
25.130357	209.518086	4.421363	-0.004434	1.058547
25.962808	218.159753	4.426368	-0.004595	1.070251
26.761625	226.812189	4.431373	-0.004749	1.081835
27.371440	235.496725	4.436378	-0.004868	1.093294
28.396996	244.132962	4.441382	-0.005064	1.104665
29.409318	252.782996	4.446387	-0.005258	1.115933
30.109121	261.462032	4.451392	-0.005394	1.127058
30.708795	270.169642	4.456397	-0.005511	1.138087
31.620590	278.811751	4.461402	-0.005686	1.148995
32.664815	287.432015	4.466406	-0.005886	1.159802
33.662631	296.021044	4.471411	-0.006077	1.170460
34.012215	304.712957	4.476416	-0.006147	1.181013
34.790946	313.325683	4.481421	-0.006298	1.191464
35.640589	321.898325	4.486426	-0.006461	1.201792
36.267846	330.523853	4.491430	-0.006584	1.212048
36.880452	339.118480	4.496435	-0.006703	1.222180
37.664448	347.690161	4.501440	-0.006854	1.232235
38.149345	356.276783	4.506445	-0.006950	1.242167
39.028895	364.773380	4.511450	-0.007119	1.251994
40.052846	373.243772	4.516454	-0.007315	1.261742
40.936109	381.746925	4.521459	-0.007485	1.271425
41.615218	390.252046	4.526464	-0.007616	1.280998
41.920896	398.829130	4.531469	-0.007679	1.290510
42.668059	407.282639	4.536474	-0.007823	1.299898
43.424858	415.790909	4.541478	-0.007969	1.309280
43.850243	424.372535	4.546483	-0.008054	1.318614
44.392381	432.784864	4.551488	-0.008160	1.327722
45.419382	441.148554	4.556493	-0.008357	1.336802
45.752617	449.587102	4.561498	-0.008424	1.345778
46.567953	457.964571	4.566502	-0.008581	1.354714
47.176757	466.351301	4.571507	-0.008699	1.363565
47.724437	474.745397	4.576512	-0.008807	1.372355
48.300253	483.131616	4.581517	-0.008919	1.381086
48.585037	491.549791	4.586522	-0.008977	1.389746
49.021314	499.939809	4.591526	-0.009064	1.398348
49.320894	508.308337	4.596531	-0.009125	1.406853
50.065471	516.614652	4.601536	-0.009269	1.415319
50.849184	524.911748	4.606541	-0.009420	1.423731
51.719603	533.192263	4.611546	-0.009587	1.432091
52.448201	541.491421	4.616550	-0.009728	1.440398
52.799500	549.847765	4.621555	-0.009798	1.448651
53.401002	558.160476	4.626560	-0.009916	1.456856
54.047739	566.458965	4.631565	-0.010041	1.465008
54.246598	574.859761	4.636570	-0.010084	1.473142
54.782792	583.143066	4.641574	-0.010189	1.481171
55.333304	591.421691	4.646579	-0.010296	1.489156
55.740130	599.712615	4.651584	-0.010377	1.497086
56.522239	607.945885	4.656589	-0.010528	1.504978
56.863232	616.250862	4.661594	-0.010597	1.512829
57.408363	624.494871	4.666598	-0.010703	1.520613
57.925724	632.749009	4.671603	-0.010805	1.528362
58.427819	640.999151	4.676608	-0.010903	1.536066
58.873077	649.265240	4.681613	-0.010991	1.543737
59.214478	657.535702	4.686618	-0.011060	1.551360
59.961208	665.742386	4.691622	-0.011204	1.558946
60.530037	673.952307	4.696627	-0.011315	1.566472
60.926926	682.209049	4.701632	-0.011394	1.573979
61.576360	690.415185	4.706637	-0.011520	1.581442
61.540990	698.714808	4.711642	-0.011519	1.588854
62.610371	706.854417	4.716646	-0.011723	1.596248
63.404783	715.031987	4.721651	-0.011876	1.603601
63.575392	723.302164	4.726656	-0.011913	1.610914
64.040018	731.542733	4.731661	-0.012005	1.618210
64.527991	739.731356	4.736666	-0.012101	1.625430
64.739042	748.040473	4.741670	-0.012145	1.632684
65.333822	756.214442	4.746675	-0.012261	1.639843
66.271140	764.313775	4.751680	-0.012440	1.646953
66.769951	772.536689	4.756685	-0.012538	1.654078
67.202607	780.716838	4.761690	-0.012624	1.661127
67.734745	788.909643	4.766694	-0.012728	1.668170
68.222207	797.120966	4.771699	-0.012824	1.675193
68.630278	805.299620	4.776704	-0.012905	1.682148
69.403147	813.451898	4.781709	-0.013054	1.689101
69.693326	821.677153	4.786714	-0.013113	1.696022
70.231731	829.841434	4.791718	-0.013219	1.702897
70.635268	838.042107	4.796723	-0.013299	1.709757
71.032097	846.237310	4.801728	-0.013378	1.716584
71.471787	854.406232	4.806733	-0.013465	1.723367
71.821742	862.571009	4.811738	-0.013535	1.730109
72.108104	870.773408	4.816742	-0.013594	1.736847
72.595049	878.916224	4.821747	-0.013689	1.743536
72.963461	887.087584	4.826752	-0.013763	1.750207
73.323585	895.279235	4.831757	-0.013835	1.756869
73.594507	903.434653	4.836762	-0.013891	1.763464
74.219375	911.558329	4.841766	-0.014012	1.770054
74.811852	919.708764	4.846771	-0.014128	1.776637
75.228352	927.850963	4.851776	-0.014210	1.783166
75.864730	936.010415	4.856781	-0.014334	1.789713
76.262906	944.207234	4.861786	-0.014413	1.796235
76.632319	952.346911	4.866790	-0.014487	1.802686
77.635540	960.408929	4.871795	-0.014679	1.809129
78.203253	968.534121	4.876800	-0.014789	1.815546
78.595232	976.703285	4.881805	-0.014867	1.821953
78.871578	984.870445	4.886810	-0.014924	1.828323
79.368646	993.029784	4.891814	-0.015022	1.834690
80.051712	1001.121187	4.896819	-0.015154	1.841005
80.282016	1009.286083	4.901824	-0.015202	1.847301
80.767811	1017.457081	4.906829	-0.015297	1.853610
80.987301	1025.614529	4.911834	-0.015343	1.859857
81.167845	1033.778428	4.916838	-0.015382	1.866082
81.552595	1041.950784	4.921843	-0.015459	1.872317
81.861318	1050.087380	4.926848	-0.015521	1.878496
82.340144	1058.183609	4.931853	-0.015616	1.884643
82.610716	1066.312551	4.936858	-0.015671	1.890771
83.284967	1074.398032	4.941862	-0.015802	1.896892
83.655618	1082.519173	4.946867	-0.015876	1.902986
83.979442	1090.656322	4.951872	-0.015941	1.909067
84.420198	1098.794855	4.956877	-0.016028	1.915142
84.541104	1106.928117	4.961882	-0.016056	1.921159
85.037790	1115.026473	4.966886	-0.016153	1.927172
85.923263	1123.097529	4.971891	-0.016323	1.933190
86.415541	1131.197472	4.976896	-0.016420	1.939167
86.877683	1139.322449	4.981901	-0.016511	1.945140
87.140295	1147.504710	4.986906	-0.016565	1.951115
87.731988	1155.620023	4.991910	-0.016680	1.957058
88.151949	1163.709838	4.996915	-0.016763	1.962947
88.459074	1171.820352	5.001920	-0.016826	1.968820
88.933980	1179.950998	5.006925	-0.016919	1.974708
89.190982	1188.048196	5.011930	-0.016972	1.980532
89.265524	1196.192473	5.016934	-0.016991	1.986352
89.816320	1204.293403	5.021939	-0.017099	1.992175
90.279467	1212.368741	5.026944	-0.017190	1.997954
90.818483	1220.455722	5.031949	-0.017295	2.003732
91.003269	1228.584638	5.036954	-0.017335	2.009485
91.320926	1236.713590	5.041958	-0.017399	2.015236
91.737790	1244.816394	5.046963	-0.017482	2.020963
91.907133	1252.931905	5.051968	-0.017518	2.026657
92.467341	1261.045970	5.056973	-0.017627	2.032373
92.917717	1269.135910	5.061978	-0.017716	2.038046
93.018182	1277.248580	5.066982	-0.017740	2.043683
93.431958	1285.350196	5.071987	-0.017822	2.049328
94.063967	1293.410562	5.076992	-0.017945	2.054951
94.379719	1301.529819	5.081997	-0.018009	2.060568
94.637723	1309.626845	5.087002	-0.018062	2.066148
94.869011	1317.759478	5.092006	-0.018110	2.071735
95.507269	1325.825154	5.097011	-0.018234	2.077301
95.744590	1333.905194	5.102016	-0.018283	2.082822
96.103299	1342.012031	5.107021	-0.018355	2.088359
96.729306	1350.078548	5.112026	-0.018476	2.093880
97.149715	1358.162168	5.117030	-0.018560	2.099378
97.665116	1366.242887	5.122035	-0.018661	2.104869
97.964755	1374.377484	5.127040	-0.018722	2.110360
98.239742	1382.549212	5.132045	-0.018778	2.115860
98.311308	1390.634421	5.137050	-0.018796	2.121268
98.949579	1398.664587	5.142054	-0.018920	2.126680
99.376824	1406.755934	5.147059	-0.019005	2.132098
99.635289	1414.848591	5.152064	-0.019058	2.137487
100.043688	1422.925962	5.157069	-0.019139	2.142867
100.515359	1430.996885	5.162074	-0.019232	2.148235
101.014442	1439.083732	5.167078	-0.019330	2.153603
101.389766	1447.172385	5.172083	-0.019405	2.158946
101.595687	1455.254445	5.177088	-0.019448	2.164256
101.661680	1463.399190	5.182093	-0.019465	2.169582
101.864088	1471.497103	5.187098	-0.019508	2.174876
102.470045	1479.527050	5.192102	-0.019626	2.180150
102.797003	1487.610932	5.197107	-0.019692	2.185421
103.052366	1495.730769	5.202112	-0.019744	2.190695
103.320504	1503.853309	5.207117	-0.019799	2.195960
103.778095	1511.871420	5.212122	-0.019890	2.201162
104.120669	1519.943568	5.217126	-0.019958	2.206376
104.353016	1528.052552	5.222131	-0.020007	2.211592
104.531616	1536.139266	5.227136	-0.020045	2.216776
105.072390	1544.197364	5.232141	-0.020151	2.221962
105.567449	1552.249655	5.237146	-0.020248	2.227128
105.898957	1560.353033	5.242150	-0.020315	2.232299
106.261929	1568.435756	5.247155	-0.020387	2.237449
106.542156	1576.491532	5.252160	-0.020445	2.242562
107.103228	1584.556984	5.257165	-0.020554	2.247694
107.494481	1592.652511	5.262170	-0.020632	2.252819
107.680845	1600.751667	5.267174	-0.020672	2.257916
108.086000	1608.810916	5.272179	-0.020752	2.262995
108.205393	1616.902934	5.277184	-0.020779	2.268059
108.694628	1625.037898	5.282189	-0.020876	2.273171
108.911968	1633.109992	5.287194	-0.020921	2.278208
109.207677	1641.154779	5.292198	-0.020981	2.283224
109.749447	1649.181013	5.297203	-0.021087	2.288238
110.181729	1657.238802	5.302208	-0.021172	2.293251
110.497816	1665.307440	5.307213	-0.021236	2.298250
110.676925	1673.394645	5.312218	-0.021275	2.303238
111.079353	1681.443168	5.317222	-0.021355	2.308210
111.326082	1689.554138	5.322227	-0.021406	2.313197
111.430506	1697.643421	5.327232	-0.021430	2.318148
111.873533	1705.686928	5.332237	-0.021518	2.323088
112.143323	1713.755052	5.337242	-0.021573	2.328019
112.572316	1721.818541	5.342246	-0.021658	2.332949
112.864133	1729.901274	5.347251	-0.021717	2.337869
113.078479	1737.966264	5.352256	-0.021762	2.342762
113.421301	1746.029297	5.357261	-0.021831	2.347653
113.679123	1754.144520	5.362266	-0.021884	2.352559
114.090934	1762.192060	5.367270	-0.021966	2.357427
114.298548	1770.260362	5.372275	-0.022009	2.362280
114.564494	1778.298101	5.377280	-0.022064	2.367110
114.988411	1786.358142	5.382285	-0.022148	2.371956
115.094028	1794.450722	5.387290	-0.022173	2.376785
115.168028	1802.521511	5.392294	-0.022191	2.381590
115.741228	1810.557565	5.397299	-0.022303	2.386404
116.042805	1818.630747	5.402304	-0.022364	2.391208
116.265389	1826.721940	5.407309	-0.022411	2.396007
116.735710	1834.744270	5.412314	-0.022503	2.400776
117.106188	1842.789532	5.417318	-0.022577	2.405540
117.352858	1850.889278	5.422323	-0.022628	2.410317
117.469810	1858.975322	5.427328	-0.022655	2.415067
118.294806	1866.969043	5.432333	-0.022814	2.419808
118.664222	1875.035043	5.437338	-0.022887	2.424547
118.869640	1883.124551	5.442342	-0.022931	2.429278
119.274567	1891.272933	5.447347	-0.023011	2.434048
119.431151	1899.317442	5.452352	-0.023045	2.438730
119.683748	1907.357599	5.457357	-0.023097	2.443408
119.804836	1915.418196	5.462362	-0.023125	2.448079
120.186488	1923.469006	5.467366	-0.023201	2.452755
120.422786	1931.539838	5.472371	-0.023250	2.457422
120.601193	1939.588373	5.477376	-0.023288	2.462063
121.145056	1947.607730	5.482381	-0.023395	2.466707
121.318423	1955.687076	5.487386	-0.023432	2.471348
121.525299	1963.767799	5.492390	-0.023475	2.475983
121.920820	1971.806413	5.497395	-0.023554	2.480600
122.316504	1979.824308	5.502400	-0.023633	2.485196
122.702989	1987.884606	5.507405	-0.023710	2.489808
123.133507	1995.942835	5.512410	-0.023795	2.494412
123.422825	2004.020977	5.517414	-0.023854	2.499009
123.589778	2012.093230	5.522419	-0.023890	2.503585
123.972099	2020.134332	5.527424	-0.023966	2.508151
124.348353	2028.232165	5.532429	-0.024041	2.512740
124.799513	2036.266789	5.537434	-0.024130	2.517291
124.912058	2044.331858	5.542438	-0.024156	2.521826
125.147277	2052.379910	5.547443	-0.024205	2.526352
125.447871	2060.428877	5.552448	-0.024266	2.530875
125.647595	2068.517078	5.557453	-0.024308	2.535404
125.739989	2076.577772	5.562458	-0.024330	2.539903
126.228648	2084.573992	5.567462	-0.024426	2.544385
126.774750	2092.622057	5.572467	-0.024533	2.548893
126.944649	2100.713589	5.577472	-0.024570	2.553390
127.497827	2108.734492	5.582477	-0.024678	2.557867
127.952457	2116.767560	5.587482	-0.024767	2.562336
128.061101	2124.852425	5.592486	-0.024793	2.566801
128.581963	2132.907384	5.597491	-0.024895	2.571271
129.032774	2140.934897	5.602496	-0.024984	2.575713
129.185497	2149.016038	5.607501	-0.025017	2.580156
129.432108	2157.065465	5.612506	-0.025068	2.584581
129.809182	2165.131064	5.617510	-0.025143	2.589015
129.973777	2173.375331	5.622515	-0.025179	2.593525
130.019562	2181.429214	5.627520	-0.025193	2.597915
130.401578	2189.403947	5.632525	-0.025269	2.602278
130.771445	2197.414244	5.637530	-0.025342	2.606652
130.987534	2205.452456	5.642534	-0.025388	2.611023
131.456337	2213.504358	5.647539	-0.025480	2.615411
131.721897	2221.510534	5.652544	-0.025534	2.619754
132.145753	2229.540979	5.657549	-0.025618	2.624112
132.386945	2237.592820	5.662554	-0.025668	2.628463
132.539348	2245.671729	5.667558	-0.025702	2.632815
132.905074	2253.723549	5.672563	-0.025775	2.637160
133.010361	2261.749467	5.677568	-0.025799	2.641466
133.163999	2269.793712	5.682573	-0.025833	2.645779
133.615199	2277.811173	5.687578	-0.025922	2.650089
134.009999	2285.872314	5.692582	-0.026001	2.654412
134.049487	2293.958868	5.697587	-0.026013	2.658718
134.586162	2301.945538	5.702592	-0.026118	2.662996
134.730302	2310.027375	5.707597	-0.026150	2.667293
135.053618	2318.104075	5.712602	-0.026215	2.671591
135.461247	2326.152420	5.717606	-0.026296	2.675873
135.797028	2334.189473	5.722611	-0.026363	2.680137
136.033901	2342.195192	5.727616	-0.026412	2.684372
136.456694	2350.233970	5.732621	-0.026496	2.688629
136.805795	2358.297611	5.737626	-0.026566	2.692888
137.196801	2366.331059	5.742630	-0.026644	2.697127
137.427097	2374.412224	5.747635	-0.026692	2.701374
137.625474	2382.432405	5.752640	-0.026734	2.705580
137.945031	2390.493746	5.757645	-0.026798	2.709809
138.012772	2398.607009	5.762650	-0.026816	2.714042
138.420418	2406.598112	5.767654	-0.026897	2.718227
138.986072	2414.606364	5.772659	-0.027007	2.722423
139.087552	2422.675979	5.777664	-0.027031	2.726616
139.173584	2430.750270	5.782669	-0.027052	2.730804
139.832819	2438.769555	5.787674	-0.027180	2.734993
140.050556	2446.797595	5.792678	-0.027225	2.739152
140.322782	2454.856362	5.797683	-0.027281	2.743325
140.590818	2462.895894	5.802688	-0.027336	2.747480
140.998165	2470.979944	5.807693	-0.027417	2.751661
141.210198	2479.114138	5.812698	-0.027461	2.755849
141.650556	2487.066966	5.817702	-0.027548	2.759952
142.016768	2495.103465	5.822707	-0.027622	2.764087
142.147631	2503.138825	5.827712	-0.027651	2.768200
142.536476	2511.190944	5.832717	-0.027728	2.772332
142.760049	2519.261725	5.837722	-0.027775	2.776457
143.233400	2527.238138	5.842726	-0.027868	2.780543
143.374638	2535.303345	5.847731	-0.027899	2.784648
143.610803	2543.350415	5.852736	-0.027948	2.788744
143.885641	2551.422858	5.857741	-0.028005	2.792848
143.882043	2559.498808	5.862746	-0.028009	2.796932
144.019070	2567.513390	5.867750	-0.028039	2.800987
144.373103	2575.533830	5.872755	-0.028110	2.805052
144.477123	2583.581266	5.877760	-0.028135	2.809110
144.757805	2591.649287	5.882765	-0.028192	2.813183
145.141062	2599.670091	5.887770	-0.028268	2.817231
145.215923	2607.721181	5.892774	-0.028287	2.821272
145.480402	2615.747807	5.897779	-0.028342	2.825305
145.681254	2623.783326	5.902784	-0.028384	2.829334
146.156883	2631.861038	5.907789	-0.028478	2.833393
146.125262	2639.919357	5.912794	-0.028477	2.837408
146.406474	2647.922139	5.917798	-0.028534	2.841407
146.958595	2655.923218	5.922803	-0.028642	2.845415
147.058768	2663.977010	5.927808	-0.028665	2.849418
147.348935	2672.040877	5.932813	-0.028725	2.853431
147.593873	2680.092964	5.937818	-0.028775	2.857430
148.003690	2688.092381	5.942822	-0.028856	2.861407
148.316391	2696.117879	5.947827	-0.028920	2.865385
148.638312	2704.144165	5.952832	-0.028985	2.869359
148.923054	2712.227188	5.957837	-0.029043	2.873353
149.248692	2720.295432	5.962842	-0.029108	2.877336
149.474886	2728.305948	5.967846	-0.029155	2.881280
149.797593	2736.346765	5.972851	-0.029220	2.885239
149.981290	2744.365772	5.977856	-0.029260	2.889174
150.169468	2752.459236	5.982861	-0.029300	2.893140
150.087172	2760.527355	5.987866	-0.029289	2.897074
150.220185	2768.547311	5.992870	-0.029319	2.900990
150.476468	2776.587662	5.997875	-0.029372	2.904918
150.819777	2784.610801	6.002880	-0.029441	2.908837
151.286602	2792.700202	6.007885	-0.029533	2.912789
151.544850	2800.755477	6.012890	-0.029586	2.916708
151.726473	2808.753358	6.017894	-0.029625	2.920590
152.116594	2816.721695	6.022899	-0.029702	2.924463
152.220497	2824.779990	6.027904	-0.029727	2.928360
152.639768	2832.825665	6.032909	-0.029810	2.932262
152.748227	2840.896050	6.037914	-0.029835	2.936154
153.080556	2848.874907	6.042918	-0.029902	2.940009
153.363517	2856.924416	6.047923	-0.029959	2.943890
153.612787	2864.951233	6.052928	-0.030011	2.947753
153.985558	2873.007313	6.057933	-0.030085	2.951631
154.150203	2881.080346	6.062938	-0.030121	2.955502
154.485226	2889.075727	6.067942	-0.030188	2.959339
155.028389	2897.106411	6.072947	-0.030294	2.963199
155.109413	2905.133254	6.077952	-0.030315	2.967028
155.185874	2913.206453	6.082957	-0.030334	2.970874
155.700748	2921.261644	6.087962	-0.030435	2.974729
155.837782	2929.274472	6.092966	-0.030465	2.978539
156.186493	2937.325808	6.097971	-0.030535	2.982374
156.349966	2945.355947	6.102976	-0.030571	2.986184
156.544432	2953.393142	6.107981	-0.030612	2.989994
156.617421	2961.492609	6.112986	-0.030630	2.993822
156.874320	2969.484329	6.117990	-0.030683	2.997604
157.338274	2977.499556	6.122995	-0.030775	3.001403
157.441952	2985.506074	6.128000	-0.030799	3.005175
157.682826	2993.532869	6.133005	-0.030849	3.008958
158.134890	3001.584324	6.138010	-0.030938	3.012758
158.268455	3009.626266	6.143014	-0.030968	3.016534
158.530094	3017.678301	6.148019	-0.031021	3.020315
158.708142	3025.694508	6.153024	-0.031060	3.024071
158.925663	3033.742758	6.158029	-0.031105	3.027840
159.375557	3041.774285	6.163034	-0.031194	3.031607
159.612898	3049.818676	6.168038	-0.031243	3.035365
159.879815	3057.841219	6.173043	-0.031298	3.039109
160.017933	3065.869651	6.178048	-0.031329	3.042846
160.248471	3073.922717	6.183053	-0.031376	3.046593
160.626143	3081.940993	6.188058	-0.031452	3.050327
160.881848	3089.981849	6.193062	-0.031504	3.054061
161.204111	3098.037334	6.198067	-0.031569	3.057800
161.247918	3106.072542	6.203072	-0.031583	3.061512
161.564297	3114.072701	6.208077	-0.031646	3.065217
161.567077	3122.160181	6.213082	-0.031652	3.068942
161.940153	3130.226533	6.218086	-0.031726	3.072670
162.490107	3138.285564	6.223091	-0.031834	3.076399
162.661017	3146.237957	6.228096	-0.031871	3.080056
162.978441	3154.246379	6.233101	-0.031935	3.083742
163.297089	3162.290356	6.238106	-0.031999	3.087439
163.597821	3170.326142	6.243110	-0.032060	3.091127
163.735284	3178.403188	6.248115	-0.032091	3.094823
163.657527	3186.424644	6.253120	-0.032081	3.098478
163.784706	3194.453476	6.258125	-0.032110	3.102142
164.377704	3202.448631	6.263130	-0.032225	3.105808
164.306884	3210.519922	6.268134	-0.032217	3.109473
164.612814	3218.578930	6.273139	-0.032279	3.113146
164.897771	3226.604242	6.278144	-0.032337	3.116798
165.183217	3234.576309	6.283149	-0.032395	3.120422
165.404118	3242.605626	6.288154	-0.032441	3.124064
165.738452	3250.625594	6.293158	-0.032509	3.127703
166.222477	3258.670045	6.298163	-0.032604	3.131356
166.259720	3266.720397	6.303168	-0.032616	3.134986
166.586798	3274.747414	6.308173	-0.032682	3.138615
167.014505	3282.778173	6.313178	-0.032766	3.142246
167.095699	3290.812785	6.318182	-0.032786	3.145859
167.435085	3298.848819	6.323187	-0.032855	3.149480
167.653398	3306.917950	6.328192	-0.032900	3.153107
167.973284	3314.956584	6.333197	-0.032965	3.156719
168.178898	3322.971001	6.338202	-0.033008	3.160312
168.343589	3330.963654	6.343206	-0.033044	3.163889
168.731899	3339.003988	6.348211	-0.033121	3.167493
168.797816	3347.047000	6.353216	-0.033138	3.171081
169.117010	3355.081036	6.358221	-0.033203	3.174671
169.515152	3363.123053	6.363226	-0.033282	3.178263
169.623206	3371.159349	6.368230	-0.033307	3.181837
169.852555	3379.170574	6.373235	-0.033355	3.185401
170.084760	3387.204012	6.378240	-0.033403	3.188971
170.346480	3395.262809	6.383245	-0.033457	3.192549
170.445748	3403.335670	6.388250	-0.033480	3.196122
170.547483	3411.313414	6.393254	-0.033504	3.199650
170.939729	3419.322006	6.398259	-0.033582	3.203199
171.110059	3427.357869	6.403264	-0.033619	3.206747
171.400683	3435.377157	6.408269	-0.033678	3.210289
171.875143	3443.422210	6.413274	-0.033771	3.213846
172.098297	3451.451712	6.418278	-0.033818	3.217382
172.183505	3459.514517	6.423283	-0.033839	3.220922
172.436240	3467.490699	6.428288	-0.033891	3.224428
172.771523	3475.531478	6.433293	-0.033958	3.227962
172.928235	3483.629346	6.438298	-0.033992	3.231509
173.110163	3491.685929	6.443302	-0.034031	3.235035
173.709485	3499.659611	6.448307	-0.034148	3.238538
173.749493	3507.679786	6.453312	-0.034160	3.242035
173.921832	3515.687784	6.458317	-0.034197	3.245528
174.239570	3523.707587	6.463322	-0.034261	3.249029
174.324925	3531.758345	6.468326	-0.034282	3.252530
174.413752	3539.823983	6.473331	-0.034304	3.256033
174.502253	3547.806871	6.478336	-0.034325	3.259497
174.937527	3555.819912	6.483341	-0.034411	3.262984
175.020168	3563.905035	6.488346	-0.034432	3.266484
175.079131	3571.906332	6.493350	-0.034448	3.269944
175.713393	3579.949889	6.498355	-0.034571	3.273440
175.498835	3588.021506	6.503360	-0.034536	3.276912
175.599499	3596.009916	6.508365	-0.034560	3.280357
175.923100	3604.046147	6.513370	-0.034625	3.283827
176.461517	3612.010604	6.518374	-0.034730	3.287271
176.336154	3620.100207	6.523379	-0.034712	3.290739
176.551865	3628.130497	6.528384	-0.034757	3.294191
176.727444	3636.159795	6.533389	-0.034795	3.297638
177.073825	3644.184494	6.538394	-0.034864	3.301085
177.051309	3652.179088	6.543398	-0.034865	3.304502
177.435650	3660.226892	6.548403	-0.034941	3.307954
177.570416	3668.292299	6.553408	-0.034972	3.311400
177.888142	3676.319171	6.558413	-0.035036	3.314833
178.303080	3684.337849	6.563418	-0.035118	3.318263
178.495867	3692.331031	6.568422	-0.035159	3.321669
178.826028	3700.345411	6.573427	-0.035225	3.325087
178.823221	3708.390113	6.578432	-0.035230	3.328501
179.023782	3716.448816	6.583437	-0.035272	3.331925
179.184013	3724.476668	6.588442	-0.035307	3.335331
179.280282	3732.496986	6.593446	-0.035330	3.338728
179.760463	3740.546759	6.598451	-0.035424	3.342149
179.950568	3748.531107	6.603456	-0.035465	3.345527
180.243180	3756.566565	6.608461	-0.035524	3.348927
180.433241	3764.649603	6.613466	-0.035565	3.352340
180.598855	3772.674079	6.618470	-0.035600	3.355724
180.842757	3780.666571	6.623475	-0.035651	3.359094
181.140902	3788.685597	6.628480	-0.035711	3.362473
181.336747	3796.703007	6.633485	-0.035753	3.365845
181.710858	3804.750552	6.638490	-0.035827	3.369233
181.641938	3812.788272	6.643494	-0.035820	3.372596
181.963453	3820.829100	6.648499	-0.035884	3.375972
181.915871	3828.848228	6.653504	-0.035881	3.379323
182.048255	3836.879486	6.658509	-0.035910	3.382681
182.701622	3844.872474	6.663514	-0.036037	3.386038
182.886280	3852.875046	6.668518	-0.036076	3.389380
183.300511	3860.994573	6.673523	-0.036158	3.392775
183.276198	3869.072161	6.678528	-0.036159	3.396133
183.560012	3877.008625	6.683533	-0.036217	3.399441
183.808747	3885.034903	6.688538	-0.036268	3.402781
183.736731	3893.043978	6.693542	-0.036260	3.406100
183.986200	3901.051418	6.698547	-0.036311	3.409425
184.344950	3909.093953	6.703552	-0.036383	3.412766
184.338366	3917.147614	6.708557	-0.036387	3.416096
184.691237	3925.125737	6.713562	-0.036457	3.419403
184.879447	3933.142743	6.718566	-0.036497	3.422718
185.128824	3941.195163	6.723571	-0.036549	3.426046
184.968701	3949.249705	6.728576	-0.036524	3.429358
185.350163	3957.266866	6.733581	-0.036600	3.432669
185.854802	3965.293291	6.738586	-0.036699	3.435986
185.904461	3973.314584	6.743590	-0.036713	3.439281
186.210206	3981.328876	6.748595	-0.036775	3.442579
186.321051	3989.353851	6.753600	-0.036801	3.445872
186.451262	3997.395674	6.758605	-0.036830	3.449169
186.794612	4005.437220	6.763610	-0.036899	3.452470
187.196679	4013.435281	6.768614	-0.036979	3.455752
187.386153	4021.488048	6.773619	-0.037019	3.459046
187.255054	4029.539811	6.778624	-0.037000	3.462326
187.475484	4037.524304	6.783629	-0.037046	3.465587
187.778487	4045.577357	6.788634	-0.037107	3.468875
187.940786	4053.605617	6.793638	-0.037142	3.472146
188.170310	4061.649262	6.798643	-0.037190	3.475422
188.469902	4069.658903	6.803648	-0.037251	3.478683
188.771072	4077.659139	6.808653	-0.037312	3.481937
188.995153	4085.670763	6.813658	-0.037359	3.485191
189.017573	4093.693481	6.818662	-0.037368	3.488439
189.242990	4101.746401	6.823667	-0.037415	3.491703
189.411078	4109.756564	6.828672	-0.037451	3.494945
189.548897	4117.758039	6.833677	-0.037482	3.498180
189.896604	4125.823463	6.838682	-0.037551	3.501443
190.143983	4133.784211	6.843686	-0.037602	3.504659
190.177800	4141.848058	6.848691	-0.037614	3.507906
190.346560	4149.916749	6.853696	-0.037650	3.511156
190.581700	4157.916374	6.858701	-0.037699	3.514378
190.966080	4165.945448	6.863706	-0.037776	3.517613
191.112070	4173.959085	6.868710	-0.037808	3.520831
191.375685	4181.959447	6.873715	-0.037862	3.524045
191.427958	4189.989589	6.878720	-0.037876	3.527261
191.627883	4198.012743	6.883725	-0.037919	3.530476
191.957991	4206.072518	6.888730	-0.037985	3.533707
192.060966	4214.115542	6.893734	-0.038009	3.536921
192.356683	4222.131817	6.898739	-0.038069	3.540128
192.542286	4230.167707	6.903744	-0.038109	3.543335
192.581366	4238.202355	6.908749	-0.038121	3.546535
192.633978	4246.247982	6.913754	-0.038136	3.549737
192.856392	4254.305517	6.918758	-0.038182	3.552946
193.020406	4262.386593	6.923763	-0.038218	3.556160
193.254390	4270.342313	6.928768	-0.038267	3.559323
193.643705	4278.308687	6.933773	-0.038344	3.562491
194.092825	4286.314203	6.938778	-0.038433	3.565675
194.216533	4294.309220	6.943782	-0.038461	3.568841
194.155566	4302.376335	6.948787	-0.038454	3.572028
194.467532	4310.394825	6.953792	-0.038517	3.575204
194.306963	4318.415559	6.958797	-0.038492	3.578364
194.719565	4326.461740	6.963802	-0.038574	3.581548
194.829417	4334.422304	6.968806	-0.038600	3.584686
195.165679	4342.475075	6.973811	-0.038667	3.587865
195.037864	4350.539318	6.978816	-0.038649	3.591032
195.143525	4358.559598	6.983821	-0.038673	3.594185
195.748701	4366.570938	6.988826	-0.038791	3.597347
195.638531	4374.541361	6.993830	-0.038775	3.600469
195.964665	4382.568758	6.998835	-0.038841	3.603623
195.940072	4390.640337	7.003840	-0.038841	3.606782
196.238011	4398.616973	7.008845	-0.038902	3.609910
196.581820	4406.669352	7.013850	-0.038971	3.613066
196.758397	4414.701567	7.018854	-0.039009	3.616207
197.232879	4422.710218	7.023859	-0.039102	3.619344
197.271677	4430.754297	7.028864	-0.039114	3.622480
197.322032	4438.741193	7.033869	-0.039129	3.625591
197.505330	4446.795517	7.038874	-0.039168	3.628730
197.838594	4454.814297	7.043878	-0.039235	3.631856
197.822396	4462.886178	7.048883	-0.039237	3.634990
198.007978	4470.913191	7.053888	-0.039276	3.638110
198.149614	4478.913169	7.058893	-0.039308	3.641215
198.456204	4486.907049	7.063898	-0.039370	3.644320
198.453174	4494.929198	7.068902	-0.039374	3.647425
198.777461	4502.968032	7.073907	-0.039440	3.650542
198.830913	4511.024339	7.078912	-0.039455	3.653657
198.724721	4519.059610	7.083917	-0.039440	3.656756
199.252430	4527.047997	7.088922	-0.039543	3.659851
199.340872	4535.062657	7.093926	-0.039565	3.662942
199.612762	4543.090378	7.098931	-0.039620	3.666040
199.815057	4551.110230	7.103936	-0.039663	3.669131
200.029977	4559.134466	7.108941	-0.039708	3.672221
200.293100	4567.189166	7.113946	-0.039762	3.675322
200.499703	4575.168301	7.118950	-0.039805	3.678389
200.985998	4583.211299	7.123955	-0.039901	3.681486
200.872118	4591.216408	7.128960	-0.039885	3.684549
201.112316	4599.234038	7.133965	-0.039934	3.687625
201.432608	4607.287477	7.138970	-0.039999	3.690713
201.427227	4615.307976	7.143974	-0.040003	3.693778
201.636993	4623.341453	7.148979	-0.040047	3.696850
201.803299	4631.314156	7.153984	-0.040083	3.699896
201.931949	4639.334477	7.158989	-0.040112	3.702957
202.242952	4647.380782	7.163994	-0.040175	3.706029
202.230473	4655.393359	7.168998	-0.040177	3.709078
202.585504	4663.435559	7.174003	-0.040249	3.712145
202.835519	4671.541498	7.179008	-0.040300	3.715231
202.734286	4679.522215	7.184013	-0.040286	3.718258
203.016686	4687.533370	7.189018	-0.040344	3.721303
203.224581	4695.465334	7.194022	-0.040387	3.724314
203.536690	4703.517586	7.199027	-0.040451	3.727371
203.976154	4711.523923	7.204032	-0.040537	3.730411
204.168779	4719.559243	7.209037	-0.040578	3.733453
204.616916	4727.643772	7.214042	-0.040667	3.736518
204.777785	4735.609249	7.219046	-0.040702	3.739528
205.020374	4743.632406	7.224051	-0.040752	3.742560
205.362987	4751.626082	7.229056	-0.040821	3.745580
205.171800	4759.667139	7.234061	-0.040790	3.748603
205.346381	4767.738350	7.239066	-0.040828	3.751644
205.599763	4775.758130	7.244070	-0.040880	3.754664
205.821343	4783.795600	7.249075	-0.040926	3.757688
205.890899	4791.783269	7.254080	-0.040944	3.760687
206.121342	4799.784961	7.259085	-0.040992	3.763693
206.495166	4807.851063	7.264090	-0.041066	3.766724
206.522402	4815.826524	7.269094	-0.041076	3.769711
206.640032	4823.918879	7.274099	-0.041103	3.772740
206.984663	4831.949721	7.279104	-0.041173	3.775750
207.126121	4839.910767	7.284109	-0.041204	3.778727
207.472235	4847.982158	7.289114	-0.041273	3.781746
207.739485	4855.939258	7.294118	-0.041328	3.784720
207.851528	4864.026029	7.299123	-0.041354	3.787735
207.918133	4872.037281	7.304128	-0.041371	3.790719
208.095597	4880.081872	7.309133	-0.041409	3.793716
208.567644	4888.116286	7.314138	-0.041502	3.796712
208.509650	4896.059916	7.319142	-0.041496	3.799661
208.600927	4904.117887	7.324147	-0.041518	3.802654
208.845814	4912.105856	7.329152	-0.041569	3.805621
208.967689	4920.126756	7.334157	-0.041597	3.808596
208.928590	4928.188678	7.339162	-0.041594	3.811580
209.364513	4936.184561	7.344166	-0.041681	3.814548
209.637950	4944.208105	7.349171	-0.041736	3.817519
209.667721	4952.211504	7.354176	-0.041747	3.820476
210.114443	4960.220832	7.359181	-0.041835	3.823442
210.292168	4968.280794	7.364186	-0.041873	3.826418
210.208954	4976.262863	7.369190	-0.041863	3.829358
210.552241	4984.325988	7.374195	-0.041932	3.832334
210.880542	4992.329328	7.379200	-0.041998	3.835285
211.091747	5000.326066	7.384205	-0.042042	3.838230
211.271537	5008.394574	7.389210	-0.042081	3.841198
211.421056	5016.335826	7.394214	-0.042113	3.844116
211.640047	5024.401907	7.399219	-0.042159	3.847079
211.681856	5032.439027	7.404224	-0.042172	3.850025
211.737564	5040.472176	7.409229	-0.042187	3.852968
211.928511	5048.519369	7.414234	-0.042228	3.855917
212.370634	5056.476957	7.419238	-0.042315	3.858836
212.740354	5064.543900	7.424243	-0.042389	3.861791
212.868987	5072.505508	7.429248	-0.042418	3.864700
212.676425	5080.576321	7.434253	-0.042387	3.867641
212.882513	5088.642648	7.439258	-0.042430	3.870586
213.067363	5096.822681	7.444262	-0.042470	3.873569
213.197511	5104.849034	7.449267	-0.042499	3.876493
213.618042	5112.762839	7.454272	-0.042582	3.879380
213.989981	5120.716267	7.459277	-0.042657	3.882277
214.157620	5128.693598	7.464282	-0.042693	3.885178
214.367075	5136.729822	7.469286	-0.042737	3.888098
214.293221	5144.758790	7.474291	-0.042728	3.891008
214.631789	5152.800392	7.479296	-0.042796	3.893928
214.583375	5160.821116	7.484301	-0.042792	3.896832
214.864099	5168.821047	7.489306	-0.042849	3.899731
215.056272	5176.824775	7.494310	-0.042890	3.902629
215.319237	5184.827395	7.499315	-0.042944	3.905525
215.286870	5192.878215	7.504320	-0.042943	3.908430
215.520542	5200.889235	7.509325	-0.042991	3.911324
215.752399	5208.947111	7.514330	-0.043040	3.914233
215.976174	5216.949071	7.519334	-0.043086	3.917119
215.901752	5224.919340	7.524339	-0.043077	3.919987
216.266430	5232.948616	7.529344	-0.043150	3.922881
216.285351	5240.960673	7.534349	-0.043159	3.925761
216.452846	5249.012867	7.539354	-0.043195	3.928655
216.754234	5257.018214	7.544358	-0.043256	3.931534
217.023176	5265.045995	7.549363	-0.043311	3.934417
217.081960	5273.079820	7.554368	-0.043327	3.937297
217.260319	5281.018538	7.559373	-0.043365	3.940143
217.730219	5289.090040	7.564378	-0.043458	3.943039
217.708429	5297.079261	7.569382	-0.043459	3.945895
217.672534	5305.116047	7.574387	-0.043457	3.948766
218.045359	5313.171906	7.579392	-0.043531	3.951648
218.310873	5321.190895	7.584397	-0.043586	3.954513
218.679850	5329.257229	7.589402	-0.043660	3.957395
218.715364	5337.191432	7.594406	-0.043671	3.960222
218.890484	5345.239533	7.599411	-0.043709	3.963090
219.002438	5353.250920	7.604416	-0.043735	3.965942
219.022516	5361.239130	7.609421	-0.043743	3.968782
219.381583	5369.299593	7.614426	-0.043815	3.971651
219.493140	5377.308264	7.619430	-0.043841	3.974495
219.734967	5385.350917	7.624435	-0.043891	3.977352
220.046065	5393.302801	7.629440	-0.043954	3.980175
220.090173	5401.338221	7.634445	-0.043967	3.983022
220.112909	5409.371587	7.639450	-0.043976	3.985866
220.128331	5417.395151	7.644454	-0.043984	3.988703
220.722439	5425.455131	7.649459	-0.044100	3.991562
220.789217	5433.506510	7.654464	-0.044117	3.994406
220.889593	5441.509909	7.659469	-0.044141	3.997232
221.298515	5449.518223	7.664474	-0.044222	4.000063
221.574479	5457.541976	7.669478	-0.044278	4.002895
221.728958	5465.544217	7.674483	-0.044312	4.005715
221.995649	5473.567527	7.679488	-0.044367	4.008543
222.126290	5481.584074	7.684493	-0.044396	4.011364
222.331877	5489.662525	7.689498	-0.044439	4.014206
222.254671	5497.672211	7.694502	-0.044430	4.017017
222.517002	5505.650197	7.699507	-0.044484	4.019821
222.903768	5513.671135	7.704512	-0.044561	4.022639
222.982462	5521.664151	7.709517	-0.044580	4.025441
223.198775	5529.724548	7.714522	-0.044626	4.028267
223.393655	5537.740760	7.719526	-0.044667	4.031075
223.462254	5545.870832	7.724531	-0.044685	4.033919
223.829066	5553.889248	7.729536	-0.044758	4.036726
224.016243	5561.767275	7.734541	-0.044798	4.039480
224.289516	5569.837726	7.739546	-0.044854	4.042300
224.244170	5577.790446	7.744550	-0.044850	4.045072
224.366444	5585.828454	7.749555	-0.044878	4.047875
224.800615	5593.879577	7.754560	-0.044964	4.050685
224.897311	5601.901269	7.759565	-0.044987	4.053477
225.110650	5609.928162	7.764570	-0.045032	4.056271
225.149165	5617.873578	7.769574	-0.045044	4.059033
225.311387	5625.938930	7.774579	-0.045079	4.061836
225.447423	5633.911103	7.779584	-0.045109	4.064604
225.746408	5641.944243	7.784589	-0.045170	4.067394
226.097653	5649.994419	7.789594	-0.045240	4.070188
226.349464	5658.010123	7.794598	-0.045292	4.072968
226.564870	5666.052739	7.799603	-0.045337	4.075754
226.788842	5674.035585	7.804608	-0.045384	4.078517
226.899920	5682.050150	7.809613	-0.045410	4.081288
227.096302	5690.071342	7.814618	-0.045451	4.084061
227.077005	5698.096661	7.819622	-0.045453	4.086830
227.321525	5706.099818	7.824627	-0.045503	4.089593
227.421193	5714.163113	7.829632	-0.045527	4.092374
227.674346	5722.147055	7.834637	-0.045579	4.095127
227.836253	5730.205361	7.839642	-0.045614	4.097902
227.869898	5738.179720	7.844646	-0.045625	4.100645
228.254638	5746.203191	7.849651	-0.045702	4.103408
228.524441	5754.235723	7.854656	-0.045757	4.106170
228.671316	5762.224773	7.859661	-0.045789	4.108914
228.918010	5770.302865	7.864666	-0.045840	4.111688
229.110935	5778.331143	7.869670	-0.045881	4.114442
229.184950	5786.358401	7.874675	-0.045900	4.117193
229.375838	5794.340178	7.879680	-0.045941	4.119927
229.496241	5802.339999	7.884685	-0.045968	4.122665
229.784986	5810.342641	7.889690	-0.046027	4.125404
229.641433	5818.382127	7.894694	-0.046005	4.128149
229.801268	5826.418586	7.899699	-0.046040	4.130894
229.960242	5834.461411	7.904704	-0.046074	4.133640
230.340387	5842.450373	7.909709	-0.046150	4.136369
230.667660	5850.470506	7.914714	-0.046216	4.139105
230.884952	5858.498181	7.919718	-0.046261	4.141841
230.909465	5866.461922	7.924723	-0.046271	4.144551
231.051435	5874.542473	7.929728	-0.046302	4.147300
231.339592	5882.525893	7.934733	-0.046361	4.150016
231.611342	5890.645840	7.939738	-0.046417	4.152777
231.544641	5898.622008	7.944742	-0.046409	4.155482
231.743009	5906.607092	7.949747	-0.046451	4.158193
231.975654	5914.649745	7.954752	-0.046499	4.160921
231.888758	5922.624778	7.959757	-0.046488	4.163621
232.079560	5930.661042	7.964762	-0.046529	4.166343
232.127590	5938.679768	7.969766	-0.046543	4.169056
232.270713	5946.707943	7.974771	-0.046574	4.171771
232.586651	5954.740269	7.979776	-0.046638	4.174488
232.935276	5962.752827	7.984781	-0.046708	4.177196
233.093834	5970.772375	7.989786	-0.046743	4.179903
233.040161	5978.761539	7.994790	-0.046738	4.182596
233.104189	5986.760343	7.999795	-0.046754	4.185292
233.319406	5994.849413	8.004800	-0.046800	4.188017
233.320592	6002.823581	8.009805	-0.046805	4.190700
233.665843	6010.961820	8.014810	-0.046874	4.193441
233.831579	6018.936516	8.019814	-0.046910	4.196122
233.942342	6026.891157	8.024819	-0.046935	4.198795
234.070578	6034.913648	8.029824	-0.046964	4.201488
234.203635	6042.853666	8.034829	-0.046994	4.204153
234.369654	6050.942183	8.039834	-0.047030	4.206865
234.416312	6058.896091	8.044838	-0.047044	4.209530
234.752490	6066.932024	8.049843	-0.047111	4.212223
234.998658	6074.973186	8.054848	-0.047162	4.214916
234.979894	6082.988378	8.059853	-0.047164	4.217595
235.146954	6091.004015	8.064858	-0.047200	4.220275
235.405814	6099.004306	8.069862	-0.047253	4.222948
235.627286	6106.990298	8.074867	-0.047299	4.225615
235.823476	6115.014021	8.079872	-0.047341	4.228292
235.786656	6123.060987	8.084877	-0.047339	4.230974
236.020631	6131.142682	8.089882	-0.047387	4.233667
236.405647	6139.132364	8.094886	-0.047464	4.236330
236.521534	6147.127449	8.099891	-0.047491	4.238990
236.678182	6155.153696	8.104896	-0.047525	4.241660
236.826092	6163.086601	8.109901	-0.047557	4.244296
237.082486	6171.185144	8.114906	-0.047610	4.246987
237.158989	6179.190410	8.119910	-0.047629	4.249644
237.451361	6187.211692	8.124915	-0.047689	4.252306
237.794325	6195.292345	8.129920	-0.047757	4.254986
237.901970	6203.277155	8.134925	-0.047782	4.257631
238.234563	6211.304287	8.139930	-0.047849	4.260291
238.263416	6219.285268	8.144934	-0.047860	4.262930
238.523027	6227.325517	8.149939	-0.047913	4.265590
238.587888	6235.333519	8.154944	-0.047930	4.268235
238.635769	6243.357379	8.159949	-0.047944	4.270884
239.013827	6251.456182	8.164954	-0.048019	4.273559
239.206075	6259.468423	8.169958	-0.048060	4.276202
239.479501	6267.416314	8.174963	-0.048116	4.278823
239.570806	6275.496206	8.179968	-0.048138	4.281485
239.759909	6283.404061	8.184973	-0.048178	4.284088
239.821969	6291.486196	8.189978	-0.048195	4.286747
239.968088	6299.459152	8.194982	-0.048227	4.289368
240.182017	6307.504779	8.199987	-0.048272	4.292013
240.364970	6315.582864	8.204992	-0.048311	4.294666
240.455543	6323.542616	8.209997	-0.048333	4.297278
240.506907	6331.589173	8.215002	-0.048347	4.299916
240.725848	6339.602361	8.220006	-0.048393	4.302543
240.882632	6347.544768	8.225011	-0.048427	4.305145
241.236394	6355.639135	8.230016	-0.048498	4.307796
241.212621	6363.566051	8.235021	-0.048499	4.310389
241.671933	6371.706275	8.240026	-0.048589	4.313053
241.595153	6379.710147	8.245030	-0.048580	4.315666
241.831843	6387.652369	8.250035	-0.048629	4.318261
241.981381	6395.711530	8.255040	-0.048662	4.320891
242.085747	6403.704845	8.260045	-0.048686	4.323498
242.251968	6411.713157	8.265050	-0.048722	4.326109
242.360814	6419.751622	8.270054	-0.048747	4.328727
242.736723	6427.745979	8.275059	-0.048822	4.331331
242.814520	6435.822825	8.280064	-0.048842	4.333959
242.577436	6443.818184	8.285069	-0.048803	4.336556
243.015985	6451.782708	8.290074	-0.048889	4.339146
243.186539	6459.832860	8.295078	-0.048926	4.341761
243.333628	6467.813355	8.300083	-0.048958	4.344351
243.450925	6475.877307	8.305088	-0.048985	4.346967
243.464635	6483.858675	8.310093	-0.048993	4.349554
243.725166	6491.942963	8.315098	-0.049046	4.352174
243.680406	6500.020049	8.320102	-0.049043	4.354788
244.189394	6507.994397	8.325107	-0.049143	4.357370
244.320479	6515.928983	8.330112	-0.049172	4.359936
244.228077	6523.957728	8.335117	-0.049160	4.362530
244.545970	6531.970709	8.340122	-0.049224	4.365119
244.590781	6539.965749	8.345126	-0.049237	4.367700
244.818376	6548.006618	8.350131	-0.049285	4.370294
245.031967	6556.036155	8.355136	-0.049330	4.372884
245.084910	6564.013422	8.360141	-0.049344	4.375454
245.332502	6572.051972	8.365146	-0.049395	4.378043
245.369937	6580.066208	8.370150	-0.049407	4.380622
245.747689	6588.065469	8.375155	-0.049483	4.383196
245.924981	6596.099396	8.380160	-0.049521	4.385779
245.927696	6604.108150	8.385165	-0.049526	4.388351
246.082684	6612.152040	8.390170	-0.049560	4.390934
246.430034	6620.154591	8.395174	-0.049630	4.393503
246.315428	6628.187365	8.400179	-0.049613	4.396078
246.504443	6636.195336	8.405184	-0.049654	4.398645
246.462106	6644.208989	8.410189	-0.049651	4.401211
246.718676	6652.204832	8.415194	-0.049703	4.403771
246.991839	6660.235436	8.420198	-0.049759	4.406341
247.281218	6668.236392	8.425203	-0.049818	4.408900
247.350216	6676.312082	8.430208	-0.049836	4.411481
247.475346	6684.293848	8.435213	-0.049864	4.414030
247.733162	6692.337932	8.440218	-0.049917	4.416598
247.879880	6700.334645	8.445222	-0.049950	4.419149
248.075257	6708.373524	8.450227	-0.049991	4.421712
248.265323	6716.350566	8.455232	-0.050031	4.424254
248.478583	6724.407470	8.460237	-0.050076	4.426820
248.626110	6732.397461	8.465242	-0.050109	4.429363
248.740599	6740.470165	8.470246	-0.050135	4.431930
248.949016	6748.496165	8.475251	-0.050179	4.434482
249.429130	6756.538834	8.480256	-0.050273	4.437039
249.416320	6764.462248	8.485261	-0.050276	4.439554
249.460807	6772.572474	8.490266	-0.050289	4.442127
249.800031	6780.449089	8.495270	-0.050357	4.444626
250.068430	6788.583494	8.500275	-0.050412	4.447205
250.032114	6796.561012	8.505280	-0.050410	4.449731
250.105611	6804.579151	8.510285	-0.050429	4.452269
250.361760	6812.605535	8.515290	-0.050482	4.454809
250.299856	6820.625717	8.520294	-0.050475	4.457344
250.494495	6828.561347	8.525299	-0.050516	4.459853
250.735870	6836.654249	8.530304	-0.050566	4.462409
250.947375	6844.598878	8.535309	-0.050611	4.464918
251.099188	6852.704190	8.540314	-0.050644	4.467475
251.225556	6860.691669	8.545318	-0.050672	4.469993
251.325157	6868.721672	8.550323	-0.050696	4.472524
251.593937	6876.754413	8.555328	-0.050751	4.475054
251.697676	6884.754894	8.560333	-0.050775	4.477572
251.965018	6892.719472	8.565338	-0.050830	4.480078
252.000588	6900.757591	8.570343	-0.050842	4.482605
252.132019	6908.735674	8.575347	-0.050871	4.485112
252.482602	6916.802613	8.580352	-0.050941	4.487646
252.644024	6924.774612	8.585357	-0.050976	4.490149
252.843966	6932.864264	8.590362	-0.051019	4.492686
252.978128	6940.847618	8.595367	-0.051049	4.495189
252.939307	6948.845052	8.600371	-0.051046	4.497695
252.921471	6956.864699	8.605376	-0.051048	4.500206
253.237849	6964.883877	8.610381	-0.051112	4.502716
253.602750	6972.894262	8.615386	-0.051185	4.505223
253.657204	6980.963832	8.620391	-0.051200	4.507745
253.618184	6988.935762	8.625395	-0.051198	4.510236
253.895551	6997.022560	8.630400	-0.051254	4.512761
253.896495	7005.006098	8.635405	-0.051259	4.515253
254.093021	7013.008574	8.640410	-0.051301	4.517749
254.311234	7020.960298	8.645415	-0.051347	4.520228
254.368694	7029.001850	8.650419	-0.051362	4.522734
254.572969	7036.998710	8.655424	-0.051405	4.525224
254.589916	7044.983289	8.660429	-0.051413	4.527709
255.016755	7053.014708	8.665434	-0.051498	4.530208
255.048770	7061.095496	8.670439	-0.051509	4.532720
255.218824	7069.101512	8.675443	-0.051546	4.535207
255.667531	7077.105268	8.680448	-0.051634	4.537693
256.155996	7085.097260	8.685453	-0.051730	4.540174
256.172506	7093.094507	8.690458	-0.051738	4.542655
256.507981	7101.121578	8.695463	-0.051806	4.545144
256.692737	7109.118711	8.700467	-0.051845	4.547622
257.034046	7117.193105	8.705472	-0.051913	4.550122
257.073523	7125.192845	8.710477	-0.051926	4.552598
257.313037	7133.278806	8.715482	-0.051975	4.555099
257.344894	7141.255092	8.720487	-0.051986	4.557565
257.543502	7149.201637	8.725491	-0.052028	4.560021
257.865449	7157.276428	8.730496	-0.052093	4.562514
257.890343	7165.206180	8.735501	-0.052103	4.564962
257.887753	7173.308367	8.740506	-0.052107	4.567461
258.031081	7181.308116	8.745511	-0.052139	4.569927
258.472982	7189.347727	8.750515	-0.052226	4.572405
258.674339	7197.362223	8.755520	-0.052269	4.574873
258.590195	7205.381986	8.760525	-0.052258	4.577341
258.830305	7213.379767	8.765530	-0.052308	4.579802
258.755590	7221.415271	8.770535	-0.052299	4.582272
258.899740	7229.351920	8.775539	-0.052331	4.584711
259.201272	7237.473505	8.780544	-0.052392	4.587206
259.337961	7245.431082	8.785549	-0.052422	4.589648
259.340223	7253.479728	8.790554	-0.052428	4.592118
259.632250	7261.547521	8.795559	-0.052487	4.594591
259.897995	7269.556640	8.800563	-0.052542	4.597046
259.926425	7277.493976	8.805568	-0.052552	4.599477
259.904248	7285.548815	8.810573	-0.052553	4.601943
260.135914	7293.511815	8.815578	-0.052601	4.604379
260.457602	7301.578130	8.820583	-0.052666	4.606846
260.353882	7309.524439	8.825587	-0.052651	4.609275
260.652271	7317.638370	8.830592	-0.052712	4.611753
260.765513	7325.648379	8.835597	-0.052738	4.614199
260.855255	7333.665756	8.840602	-0.052760	4.616645
261.276394	7341.634288	8.845607	-0.052843	4.619075
261.483553	7349.637812	8.850611	-0.052887	4.621515
261.529133	7357.697816	8.855616	-0.052900	4.623970
261.592781	7365.678045	8.860621	-0.052917	4.626400
261.977345	7373.684405	8.865626	-0.052993	4.628836
262.274539	7381.720694	8.870631	-0.053054	4.631281
262.269926	7389.742410	8.875635	-0.053058	4.633719
262.638082	7397.818321	8.880640	-0.053132	4.636173
262.539162	7405.785692	8.885645	-0.053118	4.638592
262.654144	7413.792618	8.890650	-0.053144	4.641023
262.660918	7421.787077	8.895655	-0.053151	4.643448
262.839318	7429.773787	8.900659	-0.053189	4.645869
263.032147	7437.836915	8.905664	-0.053230	4.648312
262.975143	7445.804674	8.910669	-0.053224	4.650726
263.200912	7453.850660	8.915674	-0.053271	4.653161
263.605396	7461.899473	8.920679	-0.053352	4.655596
263.634217	7469.882182	8.925683	-0.053362	4.658010
263.848560	7477.914154	8.930688	-0.053407	4.660437
264.037879	7485.909990	8.935693	-0.053447	4.662853
264.126698	7493.899305	8.940698	-0.053468	4.665265
264.117474	7501.995868	8.945703	-0.053472	4.667708
264.395878	7509.943673	8.950707	-0.053529	4.670105
264.674376	7518.022059	8.955712	-0.053585	4.672539
264.600394	7526.094789	8.960717	-0.053577	4.674972
264.591690	7534.095290	8.965722	-0.053580	4.677381
264.972778	7542.009602	8.970727	-0.053656	4.679763
264.987887	7550.010212	8.975731	-0.053664	4.682169
265.233961	7558.018318	8.980736	-0.053715	4.684577
265.453476	7566.047119	8.985741	-0.053760	4.686989
265.662781	7573.991712	8.990746	-0.053804	4.689375
265.516617	7582.103647	8.995751	-0.053782	4.691810
265.704455	7590.103222	9.000755	-0.053822	4.694210
266.035393	7598.176636	9.005760	-0.053889	4.696631
265.964067	7606.119319	9.010765	-0.053880	4.699012
266.044846	7614.182771	9.015770	-0.053900	4.701427
266.291816	7622.129572	9.020775	-0.053951	4.703806
266.350704	7630.152162	9.025779	-0.053967	4.706207
266.531875	7638.207987	9.030784	-0.054006	4.708616
266.774367	7646.214172	9.035789	-0.054056	4.711009
266.959764	7654.282602	9.040794	-0.054096	4.713420
267.061970	7662.279282	9.045799	-0.054120	4.715808
267.204659	7670.259475	9.050803	-0.054151	4.718189
267.541377	7678.275765	9.055808	-0.054219	4.720580
267.549459	7686.315391	9.060813	-0.054226	4.722978
267.422010	7694.282469	9.065818	-0.054207	4.725353
267.785611	7702.350223	9.070823	-0.054279	4.727755
268.141175	7710.348736	9.075827	-0.054351	4.730135
267.927125	7718.410037	9.080832	-0.054316	4.732535
268.027388	7726.408050	9.085837	-0.054339	4.734914
268.186522	7734.412813	9.090842	-0.054374	4.737293
268.360017	7742.378724	9.095847	-0.054411	4.739659
268.445214	7750.437161	9.100851	-0.054432	4.742052
268.610633	7758.450049	9.105856	-0.054468	4.744430
268.668809	7766.489044	9.110861	-0.054484	4.746815
268.878471	7774.473727	9.115866	-0.054528	4.749182
269.115463	7782.509142	9.120871	-0.054577	4.751563
269.141213	7790.568451	9.125875	-0.054587	4.753951
269.262663	7798.553822	9.130880	-0.054614	4.756315
269.417335	7806.530942	9.135885	-0.054648	4.758675
269.558641	7814.546770	9.140890	-0.054679	4.761045
269.753079	7822.569405	9.145895	-0.054721	4.763417
269.684894	7830.565440	9.150899	-0.054713	4.765780
269.810106	7838.576279	9.155904	-0.054741	4.768145
269.997592	7846.586647	9.160909	-0.054781	4.770509
270.055719	7854.632223	9.165914	-0.054797	4.772883
270.056489	7862.650382	9.170919	-0.054802	4.775247
270.257274	7870.633839	9.175923	-0.054844	4.777600
270.551922	7878.671328	9.180928	-0.054904	4.779967
270.627557	7886.639958	9.185933	-0.054923	4.782313
270.869178	7894.632858	9.190938	-0.054973	4.784664
270.998118	7902.746050	9.195943	-0.055002	4.787050
271.004689	7910.723545	9.200947	-0.055008	4.789396
271.134802	7918.808743	9.205952	-0.055038	4.791772
271.148983	7926.775128	9.210957	-0.055045	4.794111
271.324642	7934.841398	9.215962	-0.055083	4.796479
271.563528	7942.770070	9.220967	-0.055132	4.798804
271.771002	7950.781000	9.225971	-0.055176	4.801153
272.023030	7958.816862	9.230976	-0.055228	4.803508
272.011818	7966.800465	9.235981	-0.055231	4.805847
272.228636	7974.873646	9.240986	-0.055276	4.808210
272.417705	7982.903508	9.245991	-0.055316	4.810560
272.351835	7990.372929	9.250995	-0.055309	4.812746
272.594986	7995.114222	9.256000	-0.055357	4.814131
272.428156	7997.633396	9.261005	-0.055327	4.814869
272.744909	7999.048062	9.266010	-0.055387	4.815281
272.845714	7999.540916	9.271015	-0.055406	4.815424
272.892704	8000.416305	9.276019	-0.055415	4.815680
272.979648	8000.385665	9.281024	-0.055431	4.815671
273.053030	8000.517135	9.286029	-0.055444	4.815709
273.107554	8000.527616	9.291034	-0.055454	4.815712
273.363572	8000.439930	9.296039	-0.055502	4.815685
273.362045	8000.319203	9.301043	-0.055501	4.815650
273.271121	8000.410611	9.306048	-0.055484	4.815677
273.332044	8000.419061	9.311053	-0.055495	4.815679
273.316147	8000.481792	9.316058	-0.055492	4.815697
273.468770	8000.428728	9.321063	-0.055520	4.815681
273.454945	8000.303528	9.326067	-0.055517	4.815645
273.479568	8000.413911	9.331072	-0.055522	4.815677
273.628351	8000.447292	9.336077	-0.055549	4.815686
273.788669	8000.389014	9.341082	-0.055579	4.815668
273.753296	8000.275209	9.346087	-0.055572	4.815635
273.712897	8000.339675	9.351091	-0.055564	4.815654
274.148506	8000.341429	9.356096	-0.055645	4.815652
274.179183	8000.361133	9.361101	-0.055650	4.815658
274.351319	8000.301980	9.366106	-0.055682	4.815640
274.482090	8000.234675	9.371111	-0.055706	4.815620
274.616085	8000.384228	9.376115	-0.055731	4.815663
274.679739	8000.166306	9.381120	-0.055743	4.815599
274.586135	8000.252332	9.386125	-0.055725	4.815624
274.575245	8000.351458	9.391130	-0.055723	4.815653
274.739495	8000.172560	9.396135	-0.055753	4.815600
274.577260	8000.443298	9.401139	-0.055723	4.815680
274.778152	8000.267134	9.406144	-0.055760	4.815628
275.039773	8000.352556	9.411149	-0.055808	4.815651
274.905331	8000.167709	9.416154	-0.055783	4.815598
275.088103	8000.205918	9.421159	-0.055817	4.815608
275.057200	8000.446764	9.426163	-0.055811	4.815679
275.121187	8000.156220	9.431168	-0.055822	4.815594
274.988325	8000.305687	9.436173	-0.055797	4.815638
274.979827	8000.327955	9.441178	-0.055796	4.815645
275.278490	8000.406508	9.446183	-0.055851	4.815666
275.284045	8000.448231	9.451187	-0.055852	4.815678
275.406141	8000.329519	9.456192	-0.055874	4.815643
275.266441	8000.366732	9.461197	-0.055848	4.815655
275.303787	8000.270131	9.466202	-0.055855	4.815626
275.371619	8000.310736	9.471207	-0.055867	4.815638
275.440008	8000.416499	9.476211	-0.055880	4.815668
275.612874	8000.313568	9.481216	-0.055912	4.815637
275.489005	8000.319000	9.486221	-0.055888	4.815640
275.528806	8000.374099	9.491226	-0.055896	4.815656
275.502063	8000.279654	9.496231	-0.055890	4.815628
275.510810	8000.404736	9.501235	-0.055892	4.815665
275.683267	8000.223832	9.506240	-0.055923	4.815611
275.579929	8000.396212	9.511245	-0.055904	4.815662
275.513244	8000.291502	9.516250	-0.055891	4.815631
275.729428	8000.401818	9.521255	-0.055931	4.815663
275.794940	8000.551326	9.526259	-0.055944	4.815706
275.937514	8000.293033	9.531264	-0.055970	4.815630
275.645518	8000.429221	9.536269	-0.055915	4.815671
275.720872	8000.409071	9.541274	-0.055929	4.815665
275.789111	8000.348219	9.546279	-0.055941	4.815647
275.656769	8000.409049	9.551283	-0.055917	4.815665
275.618087	8000.222559	9.556288	-0.055909	4.815611
275.784873	8000.412170	9.561293	-0.055940	4.815665
275.816915	8000.281304	9.566298	-0.055946	4.815627
275.727064	8000.260591	9.571303	-0.055929	4.815621
275.725112	8000.553180	9.576307	-0.055928	4.815707
275.894908	8000.264360	9.581312	-0.055959	4.815622
275.771268	8000.391551	9.586317	-0.055936	4.815660
275.843538	8000.473882	9.591322	-0.055949	4.815683
275.808352	8000.209482	9.596327	-0.055943	4.815606
275.773956	8000.265504	9.601331	-0.055936	4.815623
275.808125	8000.335464	9.606336	-0.055942	4.815643
275.959918	8000.407347	9.611341	-0.055970	4.815663
276.048894	8000.335085	9.616346	-0.055986	4.815642
276.044972	8000.277326	9.621351	-0.055985	4.815625
276.087842	8000.391219	9.626355	-0.055993	4.815658
276.237771	8000.389377	9.631360	-0.056021	4.815657
276.052721	8000.426916	9.636365	-0.055986	4.815669
275.994710	8000.396042	9.641370	-0.055975	4.815660
276.065060	8000.196380	9.646375	-0.055988	4.815601
276.042786	8000.389310	9.651379	-0.055984	4.815658
276.024261	8000.147610	9.656384	-0.055980	4.815587
276.152855	8000.343006	9.661389	-0.056004	4.815644
276.147879	8000.459321	9.666394	-0.056003	4.815678
276.118471	8000.272979	9.671399	-0.055997	4.815623
276.149444	8000.350364	9.676403	-0.056002	4.815646
276.276985	8000.322523	9.681408	-0.056026	4.815637
276.209077	8000.507232	9.686413	-0.056013	4.815691
276.127504	8000.396937	9.691418	-0.055998	4.815660
276.366711	8000.254504	9.696423	-0.056042	4.815617
276.307327	8000.428672	9.701427	-0.056031	4.815668
276.158540	8000.240380	9.706432	-0.056003	4.815614
276.220707	8000.387697	9.711437	-0.056014	4.815656
276.183560	8000.361435	9.716442	-0.056007	4.815649
276.172270	8000.402884	9.721447	-0.056004	4.815661
276.083291	8000.514622	9.726451	-0.055988	4.815694
276.277657	8000.331938	9.731456	-0.056024	4.815640
276.317649	8000.459669	9.736461	-0.056031	4.815677
276.177205	8000.410358	9.741466	-0.056004	4.815663
276.266865	8000.269753	9.746471	-0.056021	4.815622
276.097619	8000.245605	9.751475	-0.055989	4.815616
276.248839	8000.234171	9.756480	-0.056017	4.815611
276.304015	8000.455070	9.761485	-0.056027	4.815676
276.391459	8000.251413	9.766490	-0.056043	4.815616
276.399319	8000.218412	9.771495	-0.056044	4.815606
276.167961	8000.387632	9.776499	-0.056001	4.815657
276.391562	8000.242808	9.781504	-0.056042	4.815613
276.207538	8000.466205	9.786509	-0.056008	4.815680
276.245291	8000.320479	9.791514	-0.056015	4.815637
276.391433	8000.352752	9.796519	-0.056042	4.815646
276.411444	8000.418210	9.801523	-0.056045	4.815665
276.416684	8000.317878	9.806528	-0.056046	4.815635
276.447620	8000.398466	9.811533	-0.056051	4.815659
276.283276	8000.395759	9.816538	-0.056021	4.815659
276.421907	8000.403345	9.821543	-0.056046	4.815660
276.205151	8000.449979	9.826547	-0.056006	4.815675
276.428775	8000.395939	9.831552	-0.056047	4.815658
276.108965	8000.462249	9.836557	-0.055987	4.815679
276.160209	8000.301791	9.841562	-0.055996	4.815632
276.484344	8000.378628	9.846567	-0.056057	4.815653
276.542494	8000.333632	9.851571	-0.056067	4.815639
276.527071	8000.208397	9.856576	-0.056064	4.815603
276.374255	8000.347929	9.861581	-0.056035	4.815644
276.452629	8000.407932	9.866586	-0.056050	4.815661
276.480301	8000.395547	9.871591	-0.056055	4.815658
276.222012	8000.519470	9.876595	-0.056006	4.815695
276.445636	8000.360761	9.881600	-0.056048	4.815648
276.558017	8000.412776	9.886605	-0.056068	4.815662
276.531462	8000.347170	9.891610	-0.056063	4.815643
276.491175	8000.267455	9.896615	-0.056055	4.815620
276.530920	8000.435768	9.901619	-0.056063	4.815669
276.690616	8000.195910	9.906624	-0.056092	4.815598
276.532912	8000.429350	9.911629	-0.056063	4.815667
276.495230	8000.376379	9.916634	-0.056055	4.815652
276.715546	8000.361803	9.921639	-0.056096	4.815647
276.537035	8000.484894	9.926643	-0.056063	4.815684
276.596352	8000.330975	9.931648	-0.056073	4.815638
276.430710	8000.496999	9.936653	-0.056042	4.815688
276.505855	8000.491798	9.941658	-0.056056	4.815686
276.561055	8000.428597	9.946663	-0.056066	4.815667
276.779732	8000.478078	9.951667	-0.056107	4.815680
276.472541	8000.397202	9.956672	-0.056049	4.815658
276.476156	8000.379084	9.961677	-0.056050	4.815653
276.700230	8000.323983	9.966682	-0.056091	4.815636
276.854106	8000.301913	9.971687	-0.056120	4.815629
276.569688	8000.271609	9.976691	-0.056066	4.815621
276.564666	8000.311024	9.981696	-0.056065	4.815633
276.522861	8000.418193	9.986701	-0.056057	4.815664
276.475539	8000.469733	9.991706	-0.056048	4.815680
276.556479	8000.290535	9.996711	-0.056063	4.815627
276.683655	8000.359881	10.001715	-0.056086	4.815646
276.757197	8000.295911	10.006720	-0.056100	4.815627
276.609257	8000.516695	10.011725	-0.056072	4.815693
276.817762	8000.493383	10.016730	-0.056111	4.815685
276.974846	8000.385920	10.021735	-0.056140	4.815653
276.336995	8000.427805	10.026739	-0.056021	4.815668
276.542112	8000.257045	10.031744	-0.056059	4.815617
276.725955	8000.303820	10.036749	-0.056093	4.815630
276.709646	8000.312077	10.041754	-0.056089	4.815632
276.660976	8000.209796	10.046759	-0.056080	4.815603
276.658915	8000.309069	10.051763	-0.056079	4.815632
276.720231	8000.325004	10.056768	-0.056091	4.815636
276.562040	8000.218796	10.061773	-0.056061	4.815606
276.556087	8000.449377	10.066778	-0.056060	4.815673
276.730188	8000.345397	10.071783	-0.056092	4.815642
276.615521	8000.475941	10.076787	-0.056070	4.815681
276.747796	8000.263403	10.081792	-0.056094	4.815618
276.867566	8000.509927	10.086797	-0.056117	4.815690
276.700700	8000.419596	10.091802	-0.056085	4.815664
276.612477	8000.405316	10.096807	-0.056069	4.815660
276.629135	8000.485672	10.101811	-0.056072	4.815684
276.760019	8000.498472	10.106816	-0.056096	4.815687
276.858078	8000.421018	10.111821	-0.056114	4.815664
276.962278	8000.400272	10.116826	-0.056133	4.815657
277.115811	8000.394217	10.121831	-0.056161	4.815655
276.841838	8000.560607	10.126835	-0.056110	4.815705
277.070610	8000.248180	10.131840	-0.056152	4.815612
276.973743	8000.413193	10.136845	-0.056134	4.815661
276.725678	8000.310854	10.141850	-0.056088	4.815632
276.805051	8000.362330	10.146855	-0.056102	4.815647
276.702125	8000.424710	10.151859	-0.056083	4.815665
276.941522	8000.242761	10.156864	-0.056127	4.815611
276.646604	8000.495320	10.161869	-0.056072	4.815686
276.761252	8000.318808	10.166874	-0.056093	4.815634
276.889000	8000.411661	10.171879	-0.056117	4.815661
276.811967	8000.314256	10.176883	-0.056102	4.815633
276.939213	8000.281069	10.181888	-0.056125	4.815622
276.830275	8000.279267	10.186893	-0.056105	4.815622
276.897673	8000.361521	10.191898	-0.056117	4.815646
276.876641	8000.267167	10.196903	-0.056113	4.815619
276.785915	8000.406646	10.201907	-0.056096	4.815660
277.009565	8000.330178	10.206912	-0.056137	4.815636
276.918465	8000.411976	10.211917	-0.056120	4.815661
276.842311	8000.347695	10.216922	-0.056106	4.815642
276.872886	8000.276614	10.221927	-0.056111	4.815621
276.923616	8000.428019	10.226931	-0.056120	4.815665
276.864669	8000.320229	10.231936	-0.056109	4.815634
277.045365	8000.457738	10.236941	-0.056143	4.815674
277.094357	8000.394435	10.241946	-0.056152	4.815655
276.965858	8000.270554	10.246951	-0.056127	4.815619
276.828224	8000.301392	10.251955	-0.056101	4.815629
277.085586	8000.219067	10.256960	-0.056149	4.815604
277.003831	8000.400347	10.261965	-0.056134	4.815657
276.812223	8000.275435	10.266970	-0.056098	4.815621
277.038752	8000.401945	10.271975	-0.056140	4.815657
277.042719	8000.388104	10.276979	-0.056140	4.815653
276.989720	8000.452369	10.281984	-0.056130	4.815672
277.180650	8000.315553	10.286989	-0.056165	4.815631
276.945677	8000.335188	10.291994	-0.056121	4.815638
277.015603	8000.173966	10.296999	-0.056134	4.815591
276.959621	8000.259542	10.302003	-0.056123	4.815616
277.015104	8000.348009	10.307008	-0.056134	4.815642
276.951831	8000.256169	10.312013	-0.056122	4.815615
276.859259	8000.226866	10.317018	-0.056104	4.815607
277.177114	8000.279036	10.322023	-0.056163	4.815621
277.098060	8000.369576	10.327027	-0.056148	4.815648
276.912796	8000.251176	10.332032	-0.056113	4.815614
277.035548	8000.401622	10.337037	-0.056136	4.815657
277.045776	8000.230879	10.342042	-0.056138	4.815607
277.079814	8000.383079	10.347047	-0.056144	4.815652
276.855432	8000.438132	10.352051	-0.056102	4.815669
277.210601	8000.270893	10.357056	-0.056168	4.815618
277.179629	8000.321633	10.362061	-0.056162	4.815633
277.057167	8000.389034	10.367066	-0.056139	4.815654
277.139934	8000.174618	10.372071	-0.056154	4.815591
277.258873	8000.448898	10.377075	-0.056176	4.815670
277.224533	8000.316944	10.382080	-0.056169	4.815632
277.137572	8000.458622	10.387085	-0.056153	4.815674
277.200160	8000.373111	10.392090	-0.056164	4.815648
277.331600	8000.219302	10.397095	-0.056188	4.815603
277.036128	8000.383204	10.402099	-0.056133	4.815652
277.163549	8000.367109	10.407104	-0.056157	4.815647
277.044504	8000.431362	10.412109	-0.056134	4.815666
276.832370	8000.422532	10.417114	-0.056094	4.815665
277.066324	8000.411384	10.422119	-0.056138	4.815660
277.122509	8000.411214	10.427123	-0.056148	4.815660
277.237510	8000.381032	10.432128	-0.056169	4.815651
277.407064	8000.468162	10.437133	-0.056201	4.815675
277.319271	8000.278725	10.442138	-0.056184	4.815620
277.196494	8000.353597	10.447143	-0.056161	4.815643
277.034221	8000.395781	10.452147	-0.056130	4.815656
277.286855	8000.264247	10.457152	-0.056177	4.815616
277.295599	8000.435260	10.462157	-0.056179	4.815666
277.138456	8000.373926	10.467162	-0.056149	4.815649
277.101144	8000.282510	10.472167	-0.056142	4.815622
277.311408	8000.400210	10.477171	-0.056181	4.815656
277.398232	8000.366363	10.482176	-0.056197	4.815646
277.191218	8000.317030	10.487181	-0.056158	4.815632
277.196713	8000.487990	10.492186	-0.056159	4.815682
277.325975	8000.260448	10.497191	-0.056182	4.815615
277.009003	8000.511580	10.502195	-0.056123	4.815690
277.218903	8000.314195	10.507200	-0.056162	4.815631
277.274800	8000.426167	10.512205	-0.056172	4.815664
277.150107	8000.382453	10.517210	-0.056149	4.815651
277.365102	8000.376335	10.522215	-0.056189	4.815649
277.287174	8000.489323	10.527219	-0.056174	4.815682
277.195582	8000.232537	10.532224	-0.056157	4.815607
277.203379	8000.292455	10.537229	-0.056158	4.815625
277.206381	8000.434536	10.542234	-0.056158	4.815666
277.304081	8000.369893	10.547239	-0.056176	4.815647
277.050702	8000.408451	10.552243	-0.056129	4.815660
277.239147	8000.248098	10.557248	-0.056163	4.815612
277.418865	8000.357822	10.562253	-0.056197	4.815643
277.101907	8000.410294	10.567258	-0.056138	4.815660
277.302354	8000.413551	10.572263	-0.056175	4.815660
277.266338	8000.505864	10.577267	-0.056168	4.815687
277.219289	8000.352339	10.582272	-0.056159	4.815642
277.132006	8000.473719	10.587277	-0.056142	4.815678
277.227913	8000.434680	10.592282	-0.056160	4.815666
277.359447	8000.284077	10.597287	-0.056184	4.815622
277.215447	8000.307335	10.602291	-0.056157	4.815629
277.287456	8000.367235	10.607296	-0.056170	4.815646
277.496997	8000.317237	10.612301	-0.056209	4.815631
277.466617	8000.393621	10.617306	-0.056203	4.815653
277.507192	8000.250074	10.622311	-0.056210	4.815611
277.298539	8000.436757	10.627315	-0.056171	4.815667
277.420351	8000.182393	10.632320	-0.056194	4.815592
277.394342	8000.401968	10.637325	-0.056189	4.815656
277.504766	8000.474246	10.642330	-0.056209	4.815677
277.428676	8000.354425	10.647335	-0.056195	4.815642
277.178426	8000.404783	10.652339	-0.056148	4.815658
277.296660	8000.393879	10.657344	-0.056170	4.815654
277.170620	8000.353347	10.662349	-0.056146	4.815643
277.445642	8000.247812	10.667354	-0.056197	4.815611
277.489428	8000.212193	10.672359	-0.056205	4.815600
277.476971	8000.392472	10.677363	-0.056202	4.815653
277.427059	8000.188703	10.682368	-0.056192	4.815594
277.423347	8000.362716	10.687373	-0.056192	4.815645
277.457849	8000.434820	10.692378	-0.056198	4.815665
277.508821	8000.397182	10.697383	-0.056207	4.815654
277.369354	8000.413038	10.702387	-0.056181	4.815660
277.283215	8000.222561	10.707392	-0.056165	4.815604
277.423721	8000.360482	10.712397	-0.056191	4.815644
277.259961	8000.310788	10.717402	-0.056160	4.815630
277.333866	8000.360039	10.722407	-0.056173	4.815644
277.299306	8000.403243	10.727411	-0.056167	4.815657
277.299759	8000.390413	10.732416	-0.056167	4.815653
277.152568	8000.412551	10.737421	-0.056139	4.815660
277.204389	8000.274529	10.742426	-0.056148	4.815620
277.422979	8000.326146	10.747431	-0.056189	4.815634
277.373992	8000.239879	10.752435	-0.056179	4.815609
277.354004	8000.326044	10.757440	-0.056175	4.815634
277.430290	8000.398831	10.762445	-0.056189	4.815655
277.358680	8000.503379	10.767450	-0.056176	4.815686
277.416661	8000.364389	10.772455	-0.056186	4.815645
277.458015	8000.365044	10.777459	-0.056194	4.815645
277.561014	8000.246016	10.782464	-0.056213	4.815610
277.488427	8000.292871	10.787469	-0.056199	4.815624
277.549908	8000.321625	10.792474	-0.056210	4.815632
277.606879	8000.381280	10.797479	-0.056221	4.815649
277.572420	8000.395649	10.802483	-0.056214	4.815654
277.392028	8000.262374	10.807488	-0.056180	4.815616
277.458319	8000.414035	10.812493	-0.056192	4.815660
277.366851	8000.391156	10.817498	-0.056175	4.815653
277.537943	8000.226247	10.822503	-0.056207	4.815604
277.623974	8000.448724	10.827507	-0.056222	4.815669
277.594301	8000.233535	10.832512	-0.056217	4.815606
277.519015	8000.325205	10.837517	-0.056202	4.815633
277.453041	8000.346535	10.842522	-0.056190	4.815640
277.502314	8000.210608	10.847527	-0.056199	4.815600
277.498068	8000.417722	10.852531	-0.056198	4.815660
277.536026	8000.228206	10.857536	-0.056204	4.815605
277.457893	8000.265358	10.862541	-0.056190	4.815616
277.455742	8000.390266	10.867546	-0.056189	4.815653
277.468314	8000.358409	10.872551	-0.056191	4.815643
277.645031	8000.457405	10.877555	-0.056224	4.815671
277.658918	8000.199138	10.882560	-0.056226	4.815596
277.495747	8000.370543	10.887565	-0.056196	4.815647
277.308066	8000.396291	10.892570	-0.056160	4.815655
277.527237	8000.409467	10.897575	-0.056201	4.815658
277.675788	8000.374494	10.902579	-0.056228	4.815647
277.550204	8000.203664	10.907584	-0.056205	4.815598
277.662875	8000.465027	10.912589	-0.056226	4.815674
277.488823	8000.414096	10.917594	-0.056193	4.815660
277.460227	8000.197859	10.922599	-0.056187	4.815596
277.419721	8000.412924	10.927603	-0.056180	4.815660
277.611223	8000.292139	10.932608	-0.056215	4.815623
277.599900	8000.305818	10.937613	-0.056213	4.815627
277.423667	8000.458854	10.942618	-0.056180	4.815673
277.797507	8000.294055	10.947623	-0.056249	4.815623
277.684015	8000.276157	10.952627	-0.056228	4.815618
277.497641	8000.317948	10.957632	-0.056193	4.815631
277.691595	8000.297601	10.962637	-0.056229	4.815625
277.724840	8000.407067	10.967642	-0.056235	4.815656
277.601250	8000.040816	10.972647	-0.056211	4.815550
277.423513	8000.339082	10.977651	-0.056178	4.815638
277.560328	8000.176816	10.982656	-0.056203	4.815590
277.569412	8000.392693	10.987661	-0.056205	4.815653
277.515387	8000.405674	10.992666	-0.056194	4.815657
277.570509	8000.252753	10.997671	-0.056204	4.815612
277.407870	8000.519226	11.002675	-0.056174	4.815691
277.368859	8000.359424	11.007680	-0.056166	4.815644
277.489155	8000.246020	11.012685	-0.056188	4.815611
277.516553	8000.177023	11.017690	-0.056193	4.815590
277.527890	8000.318172	11.022695	-0.056195	4.815631
277.655136	8000.374703	11.027699	-0.056219	4.815647
277.679687	8000.355859	11.032704	-0.056223	4.815642
277.603930	8000.417615	11.037709	-0.056209	4.815660
277.455274	8000.266702	11.042714	-0.056181	4.815617
277.705698	8000.250483	11.047719	-0.056227	4.815611
277.687937	8000.359115	11.052723	-0.056224	4.815643
277.501192	8000.304773	11.057728	-0.056189	4.815628
277.678122	8000.320462	11.062733	-0.056221	4.815631
277.666405	8000.378993	11.067738	-0.056219	4.815649
277.639483	8000.380668	11.072743	-0.056214	4.815649
277.766467	8000.482056	11.077747	-0.056237	4.815678
277.653619	8000.325318	11.082752	-0.056216	4.815633
277.629705	8000.305681	11.087757	-0.056211	4.815627
277.532673	8000.390587	11.092762	-0.056193	4.815653
277.758977	8000.371838	11.097767	-0.056235	4.815646
277.698905	8000.458417	11.102771	-0.056223	4.815672
277.610228	8000.251876	11.107776	-0.056206	4.815612
277.418304	8000.404655	11.112781	-0.056171	4.815657
277.577682	8000.397628	11.117786	-0.056200	4.815655
277.861835	8000.287970	11.122791	-0.056253	4.815621
277.511502	8000.399708	11.127795	-0.056187	4.815656
277.435761	8000.434763	11.132800	-0.056173	4.815666
277.604401	8000.311468	11.137805	-0.056204	4.815629
277.439171	8000.404871	11.142810	-0.056173	4.815657
277.658921	8000.274935	11.147815	-0.056214	4.815618
277.721042	8000.293019	11.152819	-0.056225	4.815623
277.443506	8000.294869	11.157824	-0.056173	4.815625
277.425673	8000.169593	11.162829	-0.056169	4.815589
277.393931	8000.373053	11.167834	-0.056163	4.815648
277.670577	8000.215210	11.172839	-0.056215	4.815601
277.425200	8000.220790	11.177843	-0.056169	4.815604
277.549699	8000.350972	11.182848	-0.056192	4.815641
277.799606	8000.175603	11.187853	-0.056238	4.815589
277.543978	8000.332680	11.192858	-0.056190	4.815636
277.345856	8000.265336	11.197863	-0.056153	4.815617
277.493779	8000.320069	11.202867	-0.056180	4.815632
277.420807	8000.447023	11.207872	-0.056167	4.815670
277.433343	8000.267772	11.212877	-0.056169	4.815617
277.500910	8000.376730	11.217882	-0.056181	4.815649
277.588004	8000.393087	11.222887	-0.056197	4.815653
277.621338	8000.402156	11.227891	-0.056203	4.815656
277.632467	8000.220746	11.232896	-0.056205	4.815603
277.795761	8000.404967	11.237901	-0.056235	4.815656
277.707965	8000.410987	11.242906	-0.056218	4.815658
277.657105	8000.170887	11.247911	-0.056209	4.815588
277.605424	8000.360137	11.252915	-0.056199	4.815644
277.573056	8000.353178	11.257920	-0.056193	4.815642
277.596989	8000.278784	11.262925	-0.056197	4.815620
277.707219	8000.406598	11.267930	-0.056217	4.815657
277.861597	8000.278797	11.272935	-0.056245	4.815619
277.589024	8000.397147	11.277939	-0.056195	4.815655
277.729997	8000.349232	11.282944	-0.056221	4.815640
277.837568	8000.218530	11.287949	-0.056240	4.815601
277.531497	8000.274384	11.292954	-0.056183	4.815619
277.670501	8000.249935	11.297959	-0.056209	4.815611
277.640665	8000.552759	11.302963	-0.056203	4.815700
277.554589	8000.321694	11.307968	-0.056187	4.815633
277.639864	8000.415990	11.312973	-0.056202	4.815660
277.574085	8000.374307	11.317978	-0.056190	4.815648
277.658046	8000.297690	11.322983	-0.056205	4.815625
277.752422	8000.329118	11.327987	-0.056223	4.815634
277.608086	8000.328873	11.332992	-0.056195	4.815635
277.810292	8000.323615	11.337997	-0.056233	4.815632
277.597941	8000.287011	11.343002	-0.056193	4.815622
277.850647	8000.112756	11.348007	-0.056240	4.815570
277.809897	8000.270142	11.353011	-0.056232	4.815616
277.871633	8000.428138	11.358016	-0.056243	4.815662
277.723703	8000.219560	11.363021	-0.056215	4.815602
277.564393	8000.372872	11.368026	-0.056186	4.815648
277.710254	8000.380577	11.373031	-0.056213	4.815649
277.583735	8000.409461	11.378035	-0.056189	4.815658
277.507795	8000.411402	11.383040	-0.056174	4.815659
277.942550	8000.252940	11.388045	-0.056255	4.815611
277.785109	8000.508819	11.393050	-0.056226	4.815686
277.584684	8000.253455	11.398055	-0.056188	4.815613
277.532808	8000.430953	11.403059	-0.056178	4.815665
277.578282	8000.324869	11.408064	-0.056186	4.815634
277.728521	8000.286719	11.413069	-0.056214	4.815622
277.631388	8000.363079	11.418074	-0.056196	4.815645
277.855217	8000.183010	11.423079	-0.056237	4.815591
277.790973	8000.413710	11.428083	-0.056225	4.815659
277.682735	8000.391626	11.433088	-0.056205	4.815653
277.726507	8000.375232	11.438093	-0.056213	4.815648
277.697422	8000.381144	11.443098	-0.056207	4.815650
277.537785	8000.216166	11.448103	-0.056177	4.815602
277.515793	8000.418718	11.453107	-0.056173	4.815661
277.575391	8000.401515	11.458112	-0.056183	4.815656
277.443700	8000.381183	11.463117	-0.056159	4.815651
277.366169	8000.366010	11.468122	-0.056144	4.815647
277.698817	8000.413084	11.473127	-0.056206	4.815659
277.592489	8000.496770	11.478131	-0.056186	4.815684
277.566139	8000.462140	11.483136	-0.056181	4.815674
277.698519	8000.391655	11.488141	-0.056205	4.815653
277.793499	8000.490383	11.493146	-0.056222	4.815681
277.804778	8000.378398	11.498151	-0.056224	4.815648
277.570837	8000.402321	11.503155	-0.056181	4.815656
277.657943	8000.467809	11.508160	-0.056197	4.815675
277.756084	8000.389288	11.513165	-0.056215	4.815652
277.612574	8000.414690	11.518170	-0.056188	4.815660
277.869226	8000.467999	11.523175	-0.056235	4.815674
278.044640	8000.407830	11.528179	-0.056268	4.815656
277.962360	8000.387238	11.533184	-0.056252	4.815650
277.884571	8000.393421	11.538189	-0.056237	4.815652
277.929218	8000.366361	11.543194	-0.056245	4.815644
277.882794	8000.393351	11.548199	-0.056236	4.815652
277.850775	8000.444074	11.553203	-0.056230	4.815667
278.043849	8000.263502	11.558208	-0.056266	4.815614
277.950656	8000.194669	11.563213	-0.056248	4.815594
277.637803	8000.324108	11.568218	-0.056190	4.815633
277.843827	8000.291142	11.573223	-0.056228	4.815623
278.005555	8000.308720	11.578227	-0.056258	4.815627
277.943260	8000.326905	11.583232	-0.056246	4.815633
277.898292	8000.259929	11.588237	-0.056237	4.815613
277.863398	8000.368280	11.593242	-0.056231	4.815645
278.009966	8000.293755	11.598247	-0.056258	4.815623
277.893156	8000.445627	11.603251	-0.056236	4.815668
277.871817	8000.349130	11.608256	-0.056232	4.815640
277.919712	8000.277264	11.613261	-0.056240	4.815618
277.814099	8000.411161	11.618266	-0.056220	4.815658
278.112742	8000.225907	11.623271	-0.056276	4.815602
278.078482	8000.415444	11.628275	-0.056269	4.815658
277.891444	8000.324782	11.633280	-0.056234	4.815632
277.912372	8000.165961	11.638285	-0.056238	4.815586
277.874021	8000.281732	11.643290	-0.056230	4.815620
278.056508	8000.333827	11.648295	-0.056264	4.815634
277.985002	8000.206604	11.653299	-0.056250	4.815597
278.071932	8000.359672	11.658304	-0.056266	4.815642
278.059481	8000.201372	11.663309	-0.056264	4.815596
277.793835	8000.406349	11.668314	-0.056214	4.815657
277.874818	8000.477078	11.673319	-0.056229	4.815677
278.017389	8000.444143	11.678323	-0.056255	4.815667
277.993168	8000.347599	11.683328	-0.056251	4.815639
278.041266	8000.210583	11.688333	-0.056259	4.815598
278.150676	8000.430239	11.693338	-0.056279	4.815662
278.184990	8000.301542	11.698343	-0.056286	4.815624
277.913207	8000.388930	11.703347	-0.056235	4.815651
277.919067	8000.245884	11.708352	-0.056236	4.815609
278.148096	8000.376710	11.713357	-0.056278	4.815646
278.000953	8000.414869	11.718362	-0.056250	4.815658
277.944323	8000.356246	11.723367	-0.056240	4.815641
278.014868	8000.295430	11.728371	-0.056252	4.815623
278.040328	8000.405838	11.733376	-0.056257	4.815656
278.162660	8000.317031	11.738381	-0.056280	4.815629
277.910943	8000.442131	11.743386	-0.056232	4.815667
277.994871	8000.360173	11.748391	-0.056248	4.815642
278.019549	8000.379781	11.753395	-0.056252	4.815648
278.103974	8000.380073	11.758400	-0.056268	4.815648
278.197516	8000.343131	11.763405	-0.056285	4.815636
278.020557	8000.247294	11.768410	-0.056252	4.815609
278.084773	8000.355130	11.773415	-0.056263	4.815641
278.249657	8000.444322	11.778419	-0.056294	4.815666
278.295625	8000.369219	11.783424	-0.056302	4.815644
278.044847	8000.308488	11.788429	-0.056255	4.815627
278.029886	8000.365898	11.793434	-0.056252	4.815644
278.221437	8000.186369	11.798439	-0.056288	4.815591
278.181690	8000.281825	11.803443	-0.056280	4.815619
278.195968	8000.398459	11.808448	-0.056282	4.815653
278.274307	8000.183967	11.813453	-0.056297	4.815590
278.084157	8000.301529	11.818458	-0.056261	4.815625
277.983633	8000.298796	11.823463	-0.056242	4.815625
278.171221	8000.345635	11.828467	-0.056277	4.815637
278.225651	8000.248241	11.833472	-0.056287	4.815609
278.123038	8000.161096	11.838477	-0.056267	4.815584
278.096716	8000.395621	11.843482	-0.056262	4.815652
278.272043	8000.188057	11.848487	-0.056295	4.815591
278.292561	8000.430826	11.853491	-0.056298	4.815662
278.076829	8000.199776	11.858496	-0.056258	4.815595
278.181441	8000.226032	11.863501	-0.056277	4.815602
278.141013	8000.306523	11.868506	-0.056269	4.815626
278.137608	8000.250907	11.873511	-0.056268	4.815610
278.048001	8000.370113	11.878515	-0.056252	4.815645
278.069314	8000.340535	11.883520	-0.056255	4.815636
278.074734	8000.368372	11.888525	-0.056256	4.815645
278.089319	8000.397428	11.893530	-0.056259	4.815653
278.124527	8000.297584	11.898535	-0.056265	4.815624
278.147536	8000.389794	11.903539	-0.056269	4.815651
278.020778	8000.367407	11.908544	-0.056245	4.815645
278.160194	8000.232952	11.913549	-0.056271	4.815605
278.041658	8000.316439	11.918554	-0.056248	4.815630
278.069606	8000.269880	11.923559	-0.056253	4.815616
278.152019	8000.433555	11.928563	-0.056269	4.815663
278.340846	8000.351176	11.933568	-0.056303	4.815638
278.211299	8000.264658	11.938573	-0.056279	4.815614
278.207913	8000.323326	11.943578	-0.056278	4.815631
278.219407	8000.352332	11.948583	-0.056280	4.815639
278.323626	8000.341198	11.953587	-0.056299	4.815636
278.155637	8000.332021	11.958592	-0.056268	4.815634
278.269721	8000.219582	11.963597	-0.056289	4.815600
278.338332	8000.456730	11.968602	-0.056301	4.815669
278.244905	8000.147574	11.973607	-0.056284	4.815579
278.127739	8000.251376	11.978611	-0.056262	4.815610
278.144229	8000.394747	11.983616	-0.056265	4.815652
278.248519	8000.385752	11.988621	-0.056284	4.815649
278.272528	8000.417098	11.993626	-0.056288	4.815658
278.280162	8000.149115	11.998631	-0.056289	4.815580
278.233199	8000.247657	12.003635	-0.056280	4.815609
278.210105	8000.181038	12.008640	-0.056275	4.815589
278.220386	8000.182253	12.013645	-0.056277	4.815590
278.332147	8000.359225	12.018650	-0.056298	4.815641
278.465967	8000.228950	12.023655	-0.056322	4.815602
278.287538	8000.291164	12.028659	-0.056289	4.815621
278.376125	8000.300069	12.033664	-0.056305	4.815623
278.385103	8000.269221	12.038669	-0.056307	4.815614
278.276578	8000.262084	12.043674	-0.056286	4.815613
278.357975	8000.161928	12.048679	-0.056301	4.815583
278.161946	8000.394746	12.053683	-0.056264	4.815652
278.183465	8000.396145	12.058688	-0.056268	4.815652
278.256225	8000.338570	12.063693	-0.056282	4.815635
278.162651	8000.326338	12.068698	-0.056264	4.815632
278.224469	8000.363643	12.073703	-0.056275	4.815643
278.278816	8000.192551	12.078707	-0.056285	4.815592
278.315013	8000.319155	12.083712	-0.056292	4.815629
278.181687	8000.302000	12.088717	-0.056266	4.815625
278.205934	8000.235087	12.093722	-0.056271	4.815605
278.420446	8000.284502	12.098727	-0.056310	4.815619
278.418661	8000.200074	12.103731	-0.056310	4.815594
278.310203	8000.218573	12.108736	-0.056289	4.815600
278.246844	8000.203631	12.113741	-0.056277	4.815596
278.324463	8000.419563	12.118746	-0.056292	4.815659
278.396314	8000.314977	12.123751	-0.056305	4.815628
278.375327	8000.297524	12.128755	-0.056301	4.815623
278.336998	8000.324646	12.133760	-0.056293	4.815631
278.466829	8000.196443	12.138765	-0.056317	4.815593
278.195791	8000.415218	12.143770	-0.056267	4.815658
278.125333	8000.273059	12.148775	-0.056253	4.815617
278.170216	8000.290861	12.153779	-0.056261	4.815622
278.176392	8000.357162	12.158784	-0.056262	4.815641
278.354747	8000.182758	12.163789	-0.056295	4.815589
278.391947	8000.254906	12.168794	-0.056302	4.815610
278.328189	8000.331812	12.173799	-0.056290	4.815633
278.074069	8000.290253	12.178803	-0.056242	4.815622
278.250801	8000.399930	12.183808	-0.056275	4.815653
278.334327	8000.222906	12.188813	-0.056290	4.815601
278.140738	8000.364978	12.193818	-0.056254	4.815644
278.269559	8000.300843	12.198823	-0.056278	4.815624
278.330336	8000.313565	12.203827	-0.056289	4.815628
278.255908	8000.355050	12.208832	-0.056275	4.815640
278.118165	8000.192566	12.213837	-0.056249	4.815593
278.300189	8000.317282	12.218842	-0.056282	4.815629
278.248529	8000.216017	12.223847	-0.056272	4.815600
278.139604	8000.315682	12.228851	-0.056252	4.815629
278.285644	8000.197357	12.233856	-0.056279	4.815594
278.377149	8000.150770	12.238861	-0.056296	4.815580
278.218503	8000.346816	12.243866	-0.056266	4.815638
278.362780	8000.267981	12.248871	-0.056293	4.815614
278.414815	8000.300854	12.253875	-0.056302	4.815624
278.183041	8000.386761	12.258880	-0.056259	4.815650
278.192098	8000.236289	12.263885	-0.056260	4.815606
278.191796	8000.297144	12.268890	-0.056260	4.815624
278.181714	8000.217921	12.273895	-0.056258	4.815601
278.240830	8000.323538	12.278899	-0.056268	4.815631
278.278703	8000.195967	12.283904	-0.056275	4.815594
278.466841	8000.123190	12.288909	-0.056310	4.815572
278.291047	8000.300799	12.293914	-0.056277	4.815624
278.360206	8000.111792	12.298919	-0.056290	4.815569
278.430819	8000.166330	12.303923	-0.056303	4.815584
278.062429	8000.332244	12.308928	-0.056234	4.815635
278.042111	8000.198382	12.313933	-0.056230	4.815596
278.120501	8000.433551	12.318938	-0.056244	4.815664
278.211902	8000.252384	12.323943	-0.056261	4.815611
278.288233	8000.327309	12.328947	-0.056275	4.815632
278.297840	8000.341330	12.333952	-0.056276	4.815636
278.229276	8000.219496	12.338957	-0.056263	4.815601
278.332496	8000.314086	12.343962	-0.056282	4.815628
278.287830	8000.250318	12.348967	-0.056274	4.815610
278.411173	8000.261927	12.353971	-0.056297	4.815612
278.172169	8000.415004	12.358976	-0.056252	4.815658
278.363728	8000.195957	12.363981	-0.056287	4.815593
278.414641	8000.392227	12.368986	-0.056297	4.815651
278.255619	8000.313771	12.373991	-0.056267	4.815628
278.220987	8000.347363	12.378995	-0.056260	4.815638
278.262023	8000.259363	12.384000	-0.056267	4.815612
278.517715	8000.174873	12.389005	-0.056315	4.815587
278.445608	8000.249507	12.394010	-0.056301	4.815609
278.074508	8000.373722	12.399015	-0.056232	4.815647
278.233919	8000.200076	12.404019	-0.056261	4.815595
278.333195	8000.328779	12.409024	-0.056280	4.815632
278.198551	8000.209069	12.414029	-0.056254	4.815598
278.099805	8000.424252	12.419034	-0.056236	4.815661
278.272229	8000.223049	12.424039	-0.056267	4.815602
278.328336	8000.387361	12.429043	-0.056278	4.815650
278.234971	8000.262984	12.434048	-0.056260	4.815614
278.510626	8000.343306	12.439053	-0.056311	4.815636
278.403518	8000.245406	12.444058	-0.056291	4.815608
278.414001	8000.151566	12.449063	-0.056293	4.815580
278.449645	8000.339041	12.454067	-0.056299	4.815635
278.384355	8000.247166	12.459072	-0.056287	4.815608
278.339518	8000.150286	12.464077	-0.056278	4.815580
278.264903	8000.297506	12.469082	-0.056264	4.815624
278.305384	8000.218042	12.474087	-0.056271	4.815600
278.222086	8000.181413	12.479091	-0.056255	4.815590
278.165027	8000.282994	12.484096	-0.056245	4.815620
278.422471	8000.207078	12.489101	-0.056292	4.815596
278.282876	8000.221863	12.494106	-0.056266	4.815601
278.111453	8000.385658	12.499111	-0.056234	4.815650
278.358855	8000.214519	12.504115	-0.056280	4.815599
278.274050	8000.443816	12.509120	-0.056264	4.815666
278.283159	8000.233533	12.514125	-0.056265	4.815605
278.378019	8000.486063	12.519130	-0.056283	4.815678
278.613196	8000.335017	12.524135	-0.056326	4.815633
278.311917	8000.211512	12.529139	-0.056270	4.815598
278.167012	8000.366128	12.534144	-0.056243	4.815644
278.294191	8000.284877	12.539149	-0.056266	4.815620
278.332128	8000.318587	12.544154	-0.056273	4.815630
278.314217	8000.126021	12.549159	-0.056269	4.815573
278.395873	8000.266184	12.554163	-0.056284	4.815614
278.106340	8000.432320	12.559168	-0.056230	4.815664
278.508285	8000.194284	12.564173	-0.056305	4.815592
278.193292	8000.418748	12.569178	-0.056246	4.815660
278.275321	8000.182956	12.574183	-0.056261	4.815590
278.371172	8000.100125	12.579187	-0.056278	4.815566
278.108104	8000.204746	12.584192	-0.056229	4.815597
278.427860	8000.290059	12.589197	-0.056289	4.815621
278.475572	8000.330338	12.594202	-0.056297	4.815632
278.245527	8000.191977	12.599207	-0.056254	4.815593
278.339515	8000.289620	12.604211	-0.056271	4.815621
278.358298	8000.174555	12.609216	-0.056275	4.815587
278.263683	8000.182599	12.614221	-0.056257	4.815590
278.252352	8000.385327	12.619226	-0.056255	4.815650
278.271499	8000.353577	12.624231	-0.056258	4.815640
278.293984	8000.393443	12.629235	-0.056262	4.815652
278.421555	8000.185098	12.634240	-0.056285	4.815590
278.437629	8000.275058	12.639245	-0.056288	4.815616
278.501831	8000.304925	12.644250	-0.056300	4.815625
278.364810	8000.257804	12.649255	-0.056274	4.815612
278.356974	8000.255519	12.654259	-0.056272	4.815611
278.248420	8000.391505	12.659264	-0.056252	4.815651
278.325898	8000.146026	12.664269	-0.056266	4.815579
278.278913	8000.236023	12.669274	-0.056257	4.815606
278.455159	8000.394824	12.674279	-0.056290	4.815651
278.583480	8000.503711	12.679283	-0.056313	4.815683
278.287583	8000.399518	12.684288	-0.056258	4.815654
278.367798	8000.375175	12.689293	-0.056273	4.815646
278.347496	8000.364141	12.694298	-0.056269	4.815643
278.404325	8000.284944	12.699303	-0.056279	4.815620
278.486703	8000.263841	12.704307	-0.056294	4.815613
278.487886	8000.394145	12.709312	-0.056294	4.815651
278.474099	8000.228347	12.714317	-0.056291	4.815603
278.375746	8000.234194	12.719322	-0.056273	4.815605
278.402756	8000.336082	12.724327	-0.056278	4.815635
278.537471	8000.227184	12.729331	-0.056302	4.815602
278.271746	8000.282630	12.734336	-0.056253	4.815620
278.334316	8000.232365	12.739341	-0.056264	4.815605
278.391561	8000.386015	12.744346	-0.056275	4.815649
278.459422	8000.261071	12.749351	-0.056287	4.815612
278.497138	8000.245646	12.754355	-0.056294	4.815608
278.482195	8000.230428	12.759360	-0.056291	4.815603
278.644878	8000.199957	12.764365	-0.056321	4.815594
278.461543	8000.391328	12.769370	-0.056286	4.815651
278.558826	8000.183555	12.774375	-0.056304	4.815589
278.585424	8000.156200	12.779379	-0.056309	4.815581
278.428861	8000.191001	12.784384	-0.056279	4.815592
278.476368	8000.215255	12.789389	-0.056288	4.815599
278.557470	8000.191994	12.794394	-0.056303	4.815592
278.458855	8000.295032	12.799399	-0.056284	4.815622
278.353918	8000.258049	12.804403	-0.056265	4.815612
278.428332	8000.206909	12.809408	-0.056278	4.815597
278.516328	8000.302318	12.814413	-0.056294	4.815624
278.465298	8000.335641	12.819418	-0.056285	4.815634
278.491297	8000.299731	12.824423	-0.056289	4.815624
278.609733	8000.335826	12.829427	-0.056311	4.815634
278.258734	8000.398421	12.834432	-0.056246	4.815654
278.271450	8000.242669	12.839437	-0.056248	4.815608
278.559800	8000.438551	12.844442	-0.056301	4.815664
278.462172	8000.169914	12.849447	-0.056283	4.815586
278.468796	8000.227677	12.854451	-0.056284	4.815603
278.484441	8000.328311	12.859456	-0.056286	4.815632
278.593344	8000.019263	12.864461	-0.056306	4.815541
278.441973	8000.367094	12.869466	-0.056278	4.815644
278.392581	8000.276547	12.874471	-0.056268	4.815617
278.684074	8000.270613	12.879475	-0.056323	4.815614
278.626778	8000.387144	12.884480	-0.056312	4.815649
278.601050	8000.362136	12.889485	-0.056307	4.815641
278.506016	8000.355220	12.894490	-0.056289	4.815640
278.580442	8000.405549	12.899495	-0.056302	4.815654
278.567747	8000.256857	12.904499	-0.056300	4.815611
278.383581	8000.356360	12.909504	-0.056265	4.815641
278.700372	8000.405312	12.914509	-0.056324	4.815654
278.489773	8000.399710	12.919514	-0.056285	4.815653
278.550924	8000.395349	12.924519	-0.056296	4.815651
278.831499	8000.177757	12.929523	-0.056348	4.815587
278.562639	8000.395499	12.934528	-0.056297	4.815651
278.532845	8000.169627	12.939533	-0.056291	4.815586
278.547513	8000.384529	12.944538	-0.056294	4.815648
278.692861	8000.314256	12.949543	-0.056321	4.815627
278.635273	8000.229983	12.954547	-0.056310	4.815603
278.542788	8000.340598	12.959552	-0.056292	4.815636
278.575594	8000.253531	12.964557	-0.056298	4.815610
278.486586	8000.351386	12.969562	-0.056282	4.815639
278.473649	8000.302022	12.974567	-0.056279	4.815625
278.670245	8000.230451	12.979571	-0.056315	4.815603
278.759226	8000.441231	12.984576	-0.056332	4.815664
278.538652	8000.366039	12.989581	-0.056290	4.815643
278.714276	8000.380640	12.994586	-0.056323	4.815646
278.767692	8000.400719	12.999591	-0.056332	4.815652
278.689200	8000.338533	13.004595	-0.056318	4.815634
278.673006	8000.246393	13.009600	-0.056314	4.815607
278.664811	8000.219536	13.014605	-0.056313	4.815600
278.851311	8000.405208	13.019610	-0.056347	4.815653
278.643484	8000.273617	13.024615	-0.056308	4.815616
278.792923	8000.284585	13.029619	-0.056336	4.815618
278.827664	8000.183665	13.034624	-0.056342	4.815588
278.730088	8000.146802	13.039629	-0.056323	4.815578
278.670507	8000.362627	13.044634	-0.056312	4.815641
278.755026	8000.328742	13.049639	-0.056328	4.815631
278.756638	8000.134357	13.054643	-0.056328	4.815574
278.404364	8000.366756	13.059648	-0.056262	4.815644
278.708891	8000.364240	13.064653	-0.056318	4.815642
278.602435	8000.252465	13.069658	-0.056298	4.815610
278.560461	8000.377791	13.074663	-0.056290	4.815646
278.638255	8000.281847	13.079667	-0.056305	4.815618
278.697205	8000.210161	13.084672	-0.056315	4.815597
278.688972	8000.216414	13.089677	-0.056313	4.815599
278.674950	8000.117902	13.094682	-0.056311	4.815570
278.708404	8000.212418	13.099687	-0.056317	4.815597
278.583697	8000.247741	13.104691	-0.056293	4.815608
278.409586	8000.415765	13.109696	-0.056261	4.815658
278.698140	8000.276273	13.114701	-0.056314	4.815616
278.823127	8000.387241	13.119706	-0.056337	4.815648
278.683618	8000.392415	13.124711	-0.056311	4.815650
278.626744	8000.231251	13.129715	-0.056300	4.815603
278.638905	8000.496314	13.134720	-0.056302	4.815681
278.531172	8000.262757	13.139725	-0.056282	4.815613
278.508472	8000.420441	13.144730	-0.056277	4.815659
278.659343	8000.343850	13.149735	-0.056305	4.815636
278.695783	8000.311314	13.154739	-0.056312	4.815626
278.695042	8000.168159	13.159744	-0.056311	4.815585
278.861393	8000.242420	13.164749	-0.056342	4.815606
278.923780	8000.386543	13.169754	-0.056353	4.815647
278.689839	8000.343176	13.174759	-0.056310	4.815636
278.768875	8000.206666	13.179763	-0.056324	4.815596
278.778961	8000.211082	13.184768	-0.056326	4.815597
278.718567	8000.157738	13.189773	-0.056314	4.815582
278.711704	8000.326361	13.194778	-0.056313	4.815631
278.622990	8000.085641	13.199783	-0.056296	4.815561
278.552556	8000.258564	13.204787	-0.056283	4.815612
278.491866	8000.237257	13.209792	-0.056271	4.815606
278.476458	8000.085319	13.214797	-0.056268	4.815562
278.638094	8000.294079	13.219802	-0.056298	4.815622
278.708392	8000.318705	13.224807	-0.056311	4.815629
278.648180	8000.250411	13.229811	-0.056299	4.815609
278.535408	8000.371375	13.234816	-0.056278	4.815645
278.576353	8000.174429	13.239821	-0.056285	4.815587
278.637340	8000.157249	13.244826	-0.056296	4.815582
278.736533	8000.219730	13.249831	-0.056315	4.815600
278.891749	8000.099419	13.254835	-0.056343	4.815564
278.576910	8000.392243	13.259840	-0.056285	4.815651
278.701952	8000.285323	13.264845	-0.056308	4.815619
278.608587	8000.362813	13.269850	-0.056290	4.815642
278.662526	8000.270752	13.274855	-0.056300	4.815615
278.739740	8000.198296	13.279859	-0.056314	4.815593
278.732742	8000.225931	13.284864	-0.056312	4.815601
278.638995	8000.060962	13.289869	-0.056295	4.815554
278.576176	8000.183810	13.294874	-0.056283	4.815590
278.602479	8000.382882	13.299879	-0.056287	4.815648
278.790755	8000.218252	13.304883	-0.056322	4.815599
278.577952	8000.385643	13.309888	-0.056282	4.815649
278.641337	8000.289464	13.314893	-0.056294	4.815621
278.675129	8000.422438	13.319898	-0.056300	4.815659
278.681753	8000.390483	13.324903	-0.056301	4.815650
278.828613	8000.247605	13.329907	-0.056328	4.815607
278.803356	8000.409520	13.334912	-0.056323	4.815655
278.675486	8000.218357	13.339917	-0.056299	4.815600
278.605845	8000.441494	13.344922	-0.056286	4.815665
278.666180	8000.273703	13.349927	-0.056297	4.815616
278.984494	8000.179557	13.354931	-0.056356	4.815587
278.683621	8000.366870	13.359936	-0.056300	4.815643
278.733574	8000.208522	13.364941	-0.056309	4.815596
278.690799	8000.196053	13.369946	-0.056300	4.815593
278.762168	8000.393726	13.374951	-0.056314	4.815651
278.587948	8000.383379	13.379955	-0.056281	4.815648
278.556856	8000.281382	13.384960	-0.056275	4.815619
278.660738	8000.164504	13.389965	-0.056294	4.815584
278.616602	8000.376309	13.394970	-0.056286	4.815646
278.736655	8000.422043	13.399975	-0.056308	4.815659
278.820694	8000.263184	13.404979	-0.056323	4.815612
278.777275	8000.262454	13.409984	-0.056315	4.815612
278.782107	8000.263580	13.414989	-0.056315	4.815612
278.726878	8000.396166	13.419994	-0.056305	4.815651
278.704267	8000.378686	13.424999	-0.056301	4.815646
278.773318	8000.183268	13.430003	-0.056313	4.815589
278.728234	8000.388649	13.435008	-0.056305	4.815649
278.809433	8000.217995	13.440013	-0.056319	4.815599
278.719560	8000.293406	13.445018	-0.056302	4.815621
278.660266	8000.322322	13.450023	-0.056291	4.815630
278.873730	8000.341814	13.455027	-0.056331	4.815635
278.770013	8000.337960	13.460032	-0.056311	4.815634
278.696970	8000.313247	13.465037	-0.056297	4.815627
278.693576	8000.374051	13.470042	-0.056296	4.815645
278.677648	8000.265894	13.475047	-0.056293	4.815614
278.509615	8000.157386	13.480051	-0.056262	4.815583
278.552680	8000.342846	13.485056	-0.056269	4.815637
278.585129	8000.035752	13.490061	-0.056275	4.815547
278.476941	8000.179219	13.495066	-0.056255	4.815589
278.525694	8000.176791	13.500071	-0.056264	4.815588
278.833391	8000.069654	13.505075	-0.056321	4.815556
278.822824	8000.241421	13.510080	-0.056318	4.815606
278.769001	8000.226634	13.515085	-0.056308	4.815602
278.794312	8000.260138	13.520090	-0.056313	4.815611
278.670775	8000.267709	13.525095	-0.056289	4.815614
278.747666	8000.040379	13.530099	-0.056303	4.815547
278.654111	8000.254578	13.535104	-0.056286	4.815611
278.783872	8000.206480	13.540109	-0.056310	4.815596
278.855543	8000.138207	13.545114	-0.056323	4.815576
278.745499	8000.250670	13.550119	-0.056302	4.815609
278.969391	7999.962727	13.555123	-0.056343	4.815524
278.687059	8000.421634	13.560128	-0.056291	4.815659
278.637910	8000.194376	13.565133	-0.056281	4.815593
278.622533	8000.258188	13.570138	-0.056278	4.815612
278.683542	8000.242076	13.575143	-0.056289	4.815607
278.939419	8000.314598	13.580147	-0.056337	4.815627
278.767317	8000.253017	13.585152	-0.056305	4.815610
278.895011	8000.054287	13.590157	-0.056328	4.815551
278.995608	8000.052707	13.595162	-0.056346	4.815550
278.687598	8000.145912	13.600167	-0.056289	4.815579
278.799825	8000.189381	13.605171	-0.056310	4.815591
278.806256	8000.287729	13.610176	-0.056311	4.815620
278.786016	7999.974432	13.615181	-0.056306	4.815528
278.776482	8000.187869	13.620186	-0.056305	4.815591
278.677889	8000.157398	13.625191	-0.056286	4.815582
278.843416	8000.197466	13.630195	-0.056317	4.815593
278.734715	8000.352675	13.635200	-0.056296	4.815639
278.889156	8000.109523	13.640205	-0.056325	4.815567
278.709058	8000.221909	13.645210	-0.056291	4.815601
278.643986	8000.240049	13.650215	-0.056279	4.815606
278.945732	8000.171266	13.655219	-0.056334	4.815585
278.733191	8000.278849	13.660224	-0.056295	4.815617
278.770746	8000.234583	13.665229	-0.056301	4.815604
278.833350	8000.286854	13.670234	-0.056313	4.815619
278.758614	8000.221526	13.675239	-0.056299	4.815601
278.725072	8000.243386	13.680243	-0.056292	4.815607
278.554658	8000.290778	13.685248	-0.056260	4.815622
278.703280	8000.108411	13.690253	-0.056288	4.815568
278.906763	8000.239887	13.695258	-0.056325	4.815605
278.875358	8000.227604	13.700263	-0.056319	4.815602
279.070831	8000.214759	13.705267	-0.056355	4.815597
278.634580	8000.263143	13.710272	-0.056274	4.815613
278.721164	8000.170548	13.715277	-0.056290	4.815586
278.666727	8000.001951	13.720282	-0.056279	4.815537
278.741813	8000.208226	13.725287	-0.056293	4.815597
278.825130	8000.128394	13.730291	-0.056308	4.815573
278.710322	8000.404196	13.735296	-0.056287	4.815654
278.956101	8000.345179	13.740301	-0.056332	4.815636
279.031148	8000.345317	13.745306	-0.056346	4.815636
278.931518	8000.229382	13.750311	-0.056327	4.815602
278.809302	8000.196388	13.755315	-0.056304	4.815593
278.910521	8000.376392	13.760320	-0.056323	4.815645
278.968018	8000.076114	13.765325	-0.056333	4.815557
278.764018	8000.266078	13.770330	-0.056295	4.815614
278.777330	8000.247050	13.775335	-0.056297	4.815608
278.866246	8000.147016	13.780339	-0.056314	4.815578
278.762084	8000.232874	13.785344	-0.056294	4.815604
278.899338	8000.282093	13.790349	-0.056319	4.815618
279.004859	8000.235734	13.795354	-0.056339	4.815604
278.698914	8000.330041	13.800359	-0.056282	4.815633
278.678223	8000.250644	13.805363	-0.056278	4.815610
278.736029	8000.341287	13.810368	-0.056288	4.815636
278.788067	8000.260944	13.815373	-0.056298	4.815612
278.695773	8000.339519	13.820378	-0.056280	4.815636
278.694243	8000.324520	13.825383	-0.056280	4.815631
278.789352	8000.206430	13.830387	-0.056297	4.815596
278.831384	8000.275454	13.835392	-0.056305	4.815616
278.896926	8000.311752	13.840397	-0.056317	4.815626
278.897936	8000.162216	13.845402	-0.056317	4.815583
278.823082	8000.392745	13.850407	-0.056303	4.815651
278.894804	8000.047840	13.855411	-0.056315	4.815549
278.897995	8000.390724	13.860416	-0.056316	4.815650
278.884290	8000.350960	13.865421	-0.056313	4.815638
279.057526	8000.269394	13.870426	-0.056345	4.815613
278.965902	8000.336232	13.875431	-0.056328	4.815633
278.957459	8000.110709	13.880435	-0.056326	4.815567
278.795948	8000.159314	13.885440	-0.056296	4.815582
278.842452	8000.185687	13.890445	-0.056304	4.815590
278.942192	8000.286629	13.895450	-0.056322	4.815619
278.750653	8000.306973	13.900455	-0.056287	4.815626
278.935902	8000.236285	13.905459	-0.056321	4.815604
278.883539	8000.298424	13.910464	-0.056311	4.815623
278.963990	8000.199320	13.915469	-0.056326	4.815593
279.038636	8000.268877	13.920474	-0.056339	4.815613
278.861274	8000.385580	13.925479	-0.056306	4.815648
278.861842	8000.197587	13.930483	-0.056306	4.815593
278.842686	8000.405528	13.935488	-0.056302	4.815654
278.844632	8000.168426	13.940493	-0.056302	4.815585
278.877360	8000.320607	13.945498	-0.056308	4.815629
278.830468	8000.294185	13.950503	-0.056299	4.815622
278.910605	8000.374514	13.955507	-0.056314	4.815645
278.745162	8000.431599	13.960512	-0.056283	4.815662
278.927380	8000.269006	13.965517	-0.056316	4.815614
278.797242	8000.366188	13.970522	-0.056292	4.815643
279.060988	8000.226290	13.975527	-0.056341	4.815601
279.184619	8000.267811	13.980531	-0.056364	4.815612
278.957441	8000.253393	13.985536	-0.056321	4.815609
279.040354	8000.146853	13.990541	-0.056336	4.815578
279.082460	8000.187039	13.995546	-0.056344	4.815589
278.944726	8000.291574	14.000551	-0.056318	4.815621
278.810628	8000.143034	14.005555	-0.056293	4.815578
278.938312	8000.209185	14.010560	-0.056316	4.815596
279.006298	8000.333106	14.015565	-0.056329	4.815632
278.792094	8000.189663	14.020570	-0.056289	4.815592
278.852127	8000.347631	14.025575	-0.056300	4.815637
278.932162	8000.217546	14.030579	-0.056314	4.815599
278.865002	8000.390524	14.035584	-0.056302	4.815650
278.810149	8000.205896	14.040589	-0.056291	4.815596
279.055633	8000.261158	14.045594	-0.056336	4.815611
278.883475	8000.282887	14.050599	-0.056304	4.815618
278.963974	8000.117563	14.055603	-0.056319	4.815570
278.851209	8000.266297	14.060608	-0.056298	4.815614
279.073344	8000.188735	14.065613	-0.056339	4.815590
278.796485	8000.251475	14.070618	-0.056287	4.815610
278.755069	8000.329814	14.075623	-0.056279	4.815633
278.912018	8000.178558	14.080627	-0.056308	4.815588
278.823942	8000.391780	14.085632	-0.056292	4.815651
278.814010	8000.359554	14.090637	-0.056289	4.815641
279.156792	8000.258332	14.095642	-0.056353	4.815610
279.067004	8000.167124	14.100647	-0.056336	4.815584
278.988160	8000.227762	14.105651	-0.056321	4.815602
278.839569	8000.290464	14.110656	-0.056293	4.815621
278.893332	8000.233646	14.115661	-0.056303	4.815604
278.888669	8000.110721	14.120666	-0.056302	4.815568
278.882750	8000.309265	14.125671	-0.056301	4.815626
278.889644	8000.163030	14.130675	-0.056301	4.815583
278.954467	8000.344575	14.135680	-0.056313	4.815636
278.802563	8000.186130	14.140685	-0.056285	4.815591
278.852663	8000.180520	14.145690	-0.056294	4.815589
278.777453	8000.303166	14.150695	-0.056280	4.815625
278.988446	8000.182699	14.155699	-0.056319	4.815589
279.093398	8000.171578	14.160704	-0.056338	4.815585
278.935802	8000.142278	14.165709	-0.056308	4.815577
279.036669	8000.288097	14.170714	-0.056327	4.815619
278.866206	8000.229748	14.175719	-0.056295	4.815603
279.020644	8000.114765	14.180723	-0.056323	4.815569
278.938024	8000.266128	14.185728	-0.056308	4.815613
278.856365	8000.113105	14.190733	-0.056292	4.815569
278.951344	8000.137067	14.195738	-0.056310	4.815576
278.989667	8000.195349	14.200743	-0.056317	4.815592
278.795114	8000.058638	14.205747	-0.056280	4.815553
278.788199	8000.152494	14.210752	-0.056279	4.815581
278.897699	8000.189510	14.215757	-0.056299	4.815591
278.915101	8000.027428	14.220762	-0.056302	4.815544
278.887484	8000.332424	14.225767	-0.056297	4.815633
278.945031	8000.182745	14.230771	-0.056307	4.815589
278.823003	8000.365506	14.235776	-0.056284	4.815643
278.578658	8000.121173	14.240781	-0.056238	4.815573
278.879660	8000.242494	14.245786	-0.056294	4.815607
278.753882	8000.269254	14.250791	-0.056271	4.815615
278.764553	8000.316403	14.255795	-0.056272	4.815629
278.745437	7999.494739	14.260800	-0.056268	4.815389
278.895438	7996.276315	14.265805	-0.056294	4.814447
278.876093	7990.729607	14.270810	-0.056286	4.812825
278.846280	7983.952162	14.275815	-0.056276	4.810843
278.720793	7976.680069	14.280819	-0.056248	4.808715
278.688405	7969.028919	14.285824	-0.056236	4.806475
278.549790	7961.196448	14.290829	-0.056205	4.804182
278.703144	7953.381807	14.295834	-0.056228	4.801891
278.732376	7945.363532	14.300839	-0.056228	4.799539
278.798429	7937.439105	14.305843	-0.056235	4.797214
278.443242	7929.424069	14.310848	-0.056164	4.794864
278.580737	7921.364953	14.315853	-0.056184	4.792496
278.604702	7913.392088	14.320858	-0.056183	4.790154
278.383062	7905.380381	14.325863	-0.056136	4.787800
278.385554	7897.382182	14.330867	-0.056131	4.785448
278.534194	7889.417504	14.335872	-0.056153	4.783104
278.279212	7881.410952	14.340877	-0.056100	4.780748
278.490577	7873.451739	14.345882	-0.056134	4.778403
278.533763	7865.398827	14.350887	-0.056137	4.776030
278.432259	7857.427449	14.355891	-0.056113	4.773680
278.307691	7849.353930	14.360896	-0.056084	4.771300
278.440684	7841.413583	14.365901	-0.056103	4.768956
278.444671	7833.369793	14.370906	-0.056099	4.766581
278.423871	7825.364588	14.375911	-0.056089	4.764216
278.435619	7817.416568	14.380915	-0.056086	4.761867
278.369400	7809.363890	14.385920	-0.056068	4.759487
278.170063	7801.402364	14.390925	-0.056026	4.757132
278.038168	7793.355996	14.395930	-0.055996	4.754751
278.073204	7785.303986	14.400935	-0.055997	4.752366
278.257343	7777.324015	14.405939	-0.056025	4.750001
278.042765	7769.353142	14.410944	-0.055980	4.747639
277.954356	7761.292943	14.415949	-0.055958	4.745249
278.232703	7753.358465	14.420954	-0.056005	4.742894
278.113797	7745.343882	14.425959	-0.055977	4.740515
277.886679	7737.348058	14.430963	-0.055929	4.738141
277.849090	7729.334038	14.435968	-0.055917	4.735759
277.829115	7721.325292	14.440973	-0.055908	4.733378
277.829472	7713.300849	14.445978	-0.055902	4.730991
277.826567	7705.302457	14.450983	-0.055896	4.728610
277.869165	7697.298032	14.455987	-0.055899	4.726227
277.616760	7689.296081	14.460992	-0.055846	4.723843
277.640908	7681.300662	14.465997	-0.055845	4.721460
277.969806	7673.317086	14.471002	-0.055901	4.719078
277.734875	7665.345326	14.476007	-0.055852	4.716700
277.582276	7657.338618	14.481011	-0.055818	4.714310
277.785889	7649.266734	14.486016	-0.055850	4.711899
277.851682	7641.266791	14.491021	-0.055857	4.709508
277.742711	7633.355189	14.496026	-0.055832	4.707143
277.617897	7625.247168	14.501031	-0.055803	4.704718
277.646691	7617.391630	14.506035	-0.055803	4.702366
277.400599	7609.315065	14.511040	-0.055751	4.699948
277.447355	7601.312438	14.516045	-0.055755	4.697551
277.648716	7593.307605	14.521050	-0.055787	4.695151
277.399493	7585.287301	14.526055	-0.055735	4.692746
277.385826	7577.235208	14.531059	-0.055727	4.690330
277.337142	7569.277519	14.536064	-0.055712	4.687941
277.391062	7561.271509	14.541069	-0.055717	4.685536
277.266803	7553.289381	14.546074	-0.055688	4.683137
277.307244	7545.257264	14.551079	-0.055690	4.680722
277.268527	7537.333667	14.556083	-0.055678	4.678339
277.080507	7529.297251	14.561088	-0.055637	4.675920
276.793590	7521.193091	14.566093	-0.055578	4.673480
276.958458	7513.210328	14.571098	-0.055604	4.671074
277.083501	7505.198319	14.576103	-0.055622	4.668659
276.987188	7497.188457	14.581107	-0.055598	4.666243
277.035894	7489.235080	14.586112	-0.055602	4.663843
276.879180	7481.266402	14.591117	-0.055567	4.661437
277.046493	7473.258646	14.596122	-0.055593	4.659018
276.978501	7465.233539	14.601127	-0.055575	4.656592
277.017509	7457.214024	14.606131	-0.055577	4.654167
276.712222	7449.246128	14.611136	-0.055514	4.651757
276.771200	7441.194849	14.616141	-0.055520	4.649319
276.884951	7433.205629	14.621146	-0.055535	4.646899
276.777133	7425.181888	14.626151	-0.055510	4.644468
276.547764	7417.252716	14.631155	-0.055462	4.642064
276.447184	7409.189113	14.636160	-0.055438	4.639618
276.456897	7401.246217	14.641165	-0.055434	4.637207
276.388440	7393.241548	14.646170	-0.055416	4.634776
276.459245	7385.179683	14.651175	-0.055423	4.632327
276.612272	7377.159130	14.656179	-0.055447	4.629889
276.673608	7369.182674	14.661184	-0.055453	4.627462
276.311500	7361.123857	14.666189	-0.055380	4.625010
276.281816	7353.231658	14.671194	-0.055369	4.622607
276.110694	7345.158070	14.676199	-0.055331	4.620148
276.164869	7337.184156	14.681203	-0.055336	4.617717
276.040964	7329.198033	14.686208	-0.055307	4.615282
276.131778	7321.152744	14.691213	-0.055319	4.612827
276.325490	7313.169958	14.696218	-0.055350	4.610390
276.213488	7305.158773	14.701223	-0.055323	4.607943
276.288905	7297.126238	14.706227	-0.055332	4.605488
276.124801	7289.180852	14.711232	-0.055296	4.603058
276.051441	7281.177405	14.716237	-0.055277	4.600610
276.197655	7273.232025	14.721242	-0.055299	4.598178
275.956574	7265.138491	14.726247	-0.055248	4.595699
275.870434	7257.111306	14.731251	-0.055227	4.593239
275.855280	7249.109712	14.736256	-0.055218	4.590786
275.921793	7241.143787	14.741261	-0.055225	4.588342
275.864584	7233.114228	14.746266	-0.055209	4.585878
275.683908	7225.127936	14.751271	-0.055170	4.583425
275.918075	7217.128666	14.756275	-0.055208	4.580967
275.803085	7209.163010	14.761280	-0.055181	4.578518
275.723323	7201.117342	14.766285	-0.055161	4.576044
275.978988	7193.166275	14.771290	-0.055203	4.573597
275.772581	7185.068887	14.776295	-0.055159	4.571103
275.796332	7177.127147	14.781299	-0.055158	4.568657
275.529580	7169.092538	14.786304	-0.055103	4.566180
275.714432	7161.111214	14.791309	-0.055132	4.563718
275.656446	7153.183690	14.796314	-0.055116	4.561272
275.473955	7145.139683	14.801319	-0.055076	4.558788
275.585904	7137.178622	14.806323	-0.055092	4.556329
275.519924	7129.117648	14.811328	-0.055074	4.553837
275.368355	7121.093837	14.816333	-0.055040	4.551355
275.342267	7113.079881	14.821338	-0.055030	4.548876
275.378739	7105.111314	14.826343	-0.055031	4.546409
275.406829	7097.082629	14.831347	-0.055031	4.543922
275.437109	7089.131837	14.836352	-0.055031	4.541457
275.336236	7081.062334	14.841357	-0.055007	4.538955
275.241244	7073.176348	14.846362	-0.054984	4.536508
275.273498	7065.050563	14.851367	-0.054985	4.533985
275.378555	7057.060456	14.856371	-0.054999	4.531504
275.249233	7049.102367	14.861376	-0.054969	4.529030
275.156820	7041.123338	14.866381	-0.054947	4.526549
275.116360	7033.166420	14.871386	-0.054934	4.524073
275.056218	7025.128804	14.876391	-0.054917	4.521571
275.009896	7017.117611	14.881395	-0.054903	4.519075
275.060793	7009.122146	14.886400	-0.054907	4.516584
275.169199	7001.065572	14.891405	-0.054922	4.514072
275.236726	6993.071798	14.896410	-0.054929	4.511578
274.899480	6985.005766	14.901415	-0.054860	4.509059
274.757297	6977.069649	14.906419	-0.054829	4.506580
274.770816	6969.079696	14.911424	-0.054826	4.504083
274.756684	6961.070466	14.916429	-0.054818	4.501578
274.873264	6953.081491	14.921434	-0.054834	4.499079
274.852792	6945.057298	14.926439	-0.054825	4.496567
274.729592	6937.064478	14.931443	-0.054796	4.494063
274.637755	6929.062922	14.936448	-0.054774	4.491555
274.794771	6921.040557	14.941453	-0.054797	4.489040
274.861842	6913.057354	14.946458	-0.054804	4.486536
274.646813	6905.050633	14.951463	-0.054759	4.484022
274.767152	6897.072850	14.956467	-0.054776	4.481516
274.661887	6889.097895	14.961472	-0.054751	4.479010
274.327106	6881.038602	14.966477	-0.054683	4.476474
274.461466	6873.029480	14.971482	-0.054703	4.473955
274.473876	6864.974628	14.976487	-0.054699	4.471419
274.424266	6857.041974	14.981491	-0.054685	4.468920
274.369996	6849.033622	14.986496	-0.054669	4.466396
274.250375	6841.043460	14.991501	-0.054641	4.463876
274.393828	6833.048800	14.996506	-0.054663	4.461354
274.111576	6825.048931	15.001511	-0.054605	4.458827
274.102663	6817.015776	15.006515	-0.054598	4.456290
274.093983	6809.020781	15.011520	-0.054591	4.453763
274.136748	6800.968494	15.016525	-0.054593	4.451217
274.324326	6793.039282	15.021530	-0.054623	4.448708
274.328645	6784.990683	15.026535	-0.054618	4.446160
274.197523	6777.015498	15.031539	-0.054588	4.443633
274.065935	6769.016360	15.036544	-0.054558	4.441097
273.987011	6761.008340	15.041549	-0.054538	4.438557
274.169066	6753.032808	15.046554	-0.054566	4.436027
274.196343	6744.989226	15.051559	-0.054566	4.433473
274.060934	6736.929012	15.056563	-0.054535	4.430912
273.906865	6728.990631	15.061568	-0.054501	4.428388
273.720574	6720.954280	15.066573	-0.054461	4.425831
273.860071	6712.997272	15.071578	-0.054482	4.423299
273.996046	6704.945830	15.076583	-0.054501	4.420736
274.030444	6696.993616	15.081587	-0.054502	4.418203
273.696032	6688.986036	15.086592	-0.054435	4.415648
273.589718	6680.959131	15.091597	-0.054409	4.413087
273.839728	6672.946964	15.096602	-0.054450	4.410531
273.715598	6664.950209	15.101607	-0.054422	4.407977
273.588525	6656.956242	15.106611	-0.054393	4.405422
273.507472	6649.002338	15.111616	-0.054372	4.402878
273.437466	6640.991424	15.116621	-0.054354	4.400315
273.438561	6633.040576	15.121626	-0.054349	4.397770
273.206672	6624.962833	15.126631	-0.054300	4.395182
273.528781	6616.995381	15.131635	-0.054354	4.392630
273.402005	6608.983761	15.136640	-0.054325	4.390060
273.131804	6600.976483	15.141645	-0.054270	4.387490
273.264104	6592.934806	15.146650	-0.054289	4.384909
273.157117	6584.995378	15.151655	-0.054263	4.382358
273.252321	6576.938498	15.156659	-0.054276	4.379769
273.309353	6569.023887	15.161664	-0.054281	4.377224
273.349583	6560.947352	15.166669	-0.054283	4.374625
273.307740	6552.988614	15.171674	-0.054270	4.372062
273.103952	6544.951404	15.176679	-0.054226	4.369471
273.179507	6537.006671	15.181683	-0.054235	4.366911
273.329895	6529.021594	15.186688	-0.054257	4.364336
273.220972	6520.984329	15.191693	-0.054232	4.361741
273.259983	6513.038875	15.196698	-0.054234	4.359176
273.102779	6505.030506	15.201703	-0.054199	4.356587
273.095684	6496.941913	15.206707	-0.054192	4.353972
273.003150	6488.862812	15.211712	-0.054169	4.351357
273.056249	6480.874341	15.216717	-0.054174	4.348772
272.902841	6472.964241	15.221722	-0.054140	4.346208
272.927579	6464.942500	15.226727	-0.054139	4.343609
272.836382	6456.945318	15.231731	-0.054116	4.341015
272.716785	6448.978571	15.236736	-0.054089	4.338429
272.603067	6440.933836	15.241741	-0.054062	4.335816
272.714200	6432.951596	15.246746	-0.054077	4.333223
272.583153	6424.910243	15.251751	-0.054048	4.330608
272.670855	6416.938089	15.256755	-0.054058	4.328016
272.719664	6408.925517	15.261760	-0.054062	4.325408
272.657276	6400.938460	15.266765	-0.054045	4.322807
272.567049	6392.955914	15.271770	-0.054023	4.320205
272.386493	6384.942945	15.276775	-0.053984	4.317591
272.407129	6376.970474	15.281779	-0.053982	4.314990
272.532296	6368.938251	15.286784	-0.054000	4.312369
272.541017	6360.874410	15.291789	-0.053996	4.309735
272.705327	6352.968447	15.296794	-0.054021	4.307152
272.414813	6344.888997	15.301799	-0.053962	4.304507
272.198492	6336.952108	15.306803	-0.053916	4.301908
272.216381	6328.948701	15.311808	-0.053914	4.299287
272.161130	6320.898609	15.316813	-0.053898	4.296649
272.198661	6312.949272	15.321818	-0.053900	4.294043
271.980790	6304.871204	15.326823	-0.053854	4.291392
272.129587	6296.891791	15.331827	-0.053876	4.288773
272.173934	6288.911265	15.336832	-0.053879	4.286153
272.022092	6280.905430	15.341837	-0.053845	4.283520
272.250084	6272.949015	15.346842	-0.053882	4.280905
272.247979	6264.916968	15.351847	-0.053876	4.278262
271.921603	6256.963674	15.356851	-0.053810	4.275641
271.930162	6248.878797	15.361856	-0.053806	4.272977
271.935267	6240.815151	15.366861	-0.053801	4.270319
271.939474	6232.903202	15.371866	-0.053797	4.267709
271.807180	6224.858849	15.376871	-0.053767	4.265052
271.697778	6216.921008	15.381875	-0.053741	4.262429
271.913813	6208.899995	15.386880	-0.053776	4.259780
271.671470	6200.957700	15.391885	-0.053725	4.257152
271.840799	6192.882759	15.396890	-0.053751	4.254481
271.799444	6184.896872	15.401895	-0.053738	4.251836
271.620892	6176.857618	15.406899	-0.053699	4.249171
271.500146	6168.919776	15.411904	-0.053671	4.246538
271.530327	6160.877295	15.416909	-0.053672	4.243871
271.662846	6152.952611	15.421914	-0.053691	4.241241
271.378201	6144.925371	15.426919	-0.053632	4.238572
271.500429	6136.947021	15.431923	-0.053650	4.235922
271.355933	6128.893127	15.436928	-0.053617	4.233242
271.135758	6120.889746	15.441933	-0.053571	4.230576
271.296585	6112.915950	15.446938	-0.053595	4.227923
271.263993	6104.881627	15.451943	-0.053584	4.225245
271.290584	6096.929288	15.456947	-0.053583	4.222594
271.372842	6088.926020	15.461952	-0.053593	4.219925
271.378326	6080.941319	15.466957	-0.053589	4.217259
271.244045	6072.940680	15.471962	-0.053558	4.214585
270.908780	6064.944771	15.476967	-0.053490	4.211909
270.930807	6056.903940	15.481971	-0.053489	4.209220
271.142947	6048.895947	15.486976	-0.053523	4.206542
270.953666	6040.897991	15.491981	-0.053482	4.203861
270.915972	6032.966605	15.496986	-0.053470	4.201203
271.056138	6024.945321	15.501991	-0.053491	4.198514
271.114431	6016.962411	15.506995	-0.053496	4.195836
271.048946	6008.887204	15.512000	-0.053478	4.193124
271.075192	6000.793883	15.517005	-0.053478	4.190405
271.063865	5992.851840	15.522010	-0.053470	4.187735
270.745166	5984.853405	15.527015	-0.053405	4.185041
270.769783	5976.911179	15.532019	-0.053405	4.182367
270.999460	5968.884843	15.537024	-0.053442	4.179666
270.739844	5960.929755	15.542029	-0.053388	4.176982
270.628875	5952.923143	15.547034	-0.053362	4.174280
270.661252	5944.881843	15.552039	-0.053363	4.171566
270.568244	5936.840740	15.557043	-0.053340	4.168850
270.431491	5928.880283	15.562048	-0.053309	4.166158
270.392108	5920.870044	15.567053	-0.053296	4.163448
270.373064	5912.909543	15.572058	-0.053287	4.160755
270.234482	5904.932511	15.577063	-0.053256	4.158052
270.311079	5896.907241	15.582067	-0.053265	4.155333
270.452547	5888.895993	15.587072	-0.053286	4.152619
270.473907	5880.828815	15.592077	-0.053284	4.149882
270.186482	5872.914781	15.597082	-0.053225	4.147192
270.336800	5864.867441	15.602087	-0.053248	4.144460
270.408770	5856.891484	15.607091	-0.053256	4.141749
270.270752	5848.910793	15.612096	-0.053225	4.139033
270.177331	5840.867789	15.617101	-0.053202	4.136294
270.278013	5832.855223	15.622106	-0.053215	4.133566
270.125186	5824.838799	15.627111	-0.053181	4.130832
269.983752	5816.875836	15.632115	-0.053149	4.128114
270.147179	5808.863109	15.637120	-0.053174	4.125381
270.127911	5800.884299	15.642125	-0.053165	4.122656
269.847598	5792.906758	15.647130	-0.053108	4.119926
269.874970	5784.925902	15.652135	-0.053107	4.117197
270.028160	5776.903670	15.657139	-0.053130	4.114454
270.035268	5768.836636	15.662144	-0.053126	4.111692
269.797622	5760.847135	15.667149	-0.053076	4.108951
269.873348	5752.898481	15.672154	-0.053085	4.106226
269.800751	5744.871611	15.677159	-0.053066	4.103471
269.663695	5736.885369	15.682163	-0.053035	4.100727
269.770459	5728.931457	15.687168	-0.053050	4.097996
269.518713	5720.875994	15.692173	-0.052997	4.095223
269.565996	5712.895172	15.697178	-0.053001	4.092478
269.547298	5704.820749	15.702183	-0.052992	4.089697
269.482817	5696.900391	15.707187	-0.052974	4.086968
269.451362	5688.937882	15.712192	-0.052963	4.084222
269.494761	5680.936155	15.717197	-0.052966	4.081463
269.539287	5672.949731	15.722202	-0.052968	4.078706
269.472646	5664.935214	15.727207	-0.052951	4.075937
269.301747	5656.895176	15.732211	-0.052913	4.073155
269.423601	5648.881320	15.737216	-0.052930	4.070384
269.310388	5640.894174	15.742221	-0.052904	4.067618
269.402303	5632.908625	15.747226	-0.052916	4.064853
269.289236	5624.954917	15.752231	-0.052889	4.062095
269.337642	5616.922616	15.757235	-0.052893	4.059309
269.334886	5608.971669	15.762240	-0.052887	4.056549
269.114643	5600.897738	15.767245	-0.052840	4.053742
269.160405	5592.894676	15.772250	-0.052843	4.050961
269.127940	5584.913851	15.777255	-0.052832	4.048184
269.042537	5576.915655	15.782259	-0.052810	4.045399
269.275100	5568.948032	15.787264	-0.052848	4.042627
269.153268	5560.908679	15.792269	-0.052820	4.039823
269.105046	5552.983662	15.797274	-0.052806	4.037059
268.938894	5544.904649	15.802279	-0.052769	4.034236
268.895504	5536.834099	15.807283	-0.052756	4.031417
268.732365	5528.867289	15.812288	-0.052720	4.028630
268.775603	5520.844415	15.817293	-0.052723	4.025824
268.734845	5512.919973	15.822298	-0.052710	4.023050
268.646304	5504.889961	15.827303	-0.052688	4.020236
268.587894	5496.926613	15.832307	-0.052671	4.017444
268.594180	5488.922359	15.837312	-0.052667	4.014637
268.526742	5480.873646	15.842317	-0.052649	4.011811
268.558660	5472.881280	15.847322	-0.052650	4.009004
268.491705	5464.889187	15.852327	-0.052632	4.006194
268.684865	5456.906955	15.857331	-0.052662	4.003390
268.506205	5448.928496	15.862336	-0.052623	4.000579
268.396397	5440.926894	15.867341	-0.052598	3.997758
268.373276	5432.941191	15.872346	-0.052588	3.994943
268.373029	5424.864524	15.877351	-0.052582	3.992095
268.247763	5416.878092	15.882355	-0.052553	3.989274
268.349543	5408.873592	15.887360	-0.052567	3.986448
268.179968	5400.889129	15.892365	-0.052530	3.983623
268.325901	5392.904486	15.897370	-0.052552	3.980801
268.248217	5384.931537	15.902375	-0.052532	3.977977
268.354794	5376.903625	15.907379	-0.052546	3.975135
268.505627	5368.896050	15.912384	-0.052569	3.972299
268.039606	5360.892654	15.917389	-0.052477	3.969452
268.133851	5352.944961	15.922394	-0.052489	3.966632
268.151791	5344.949439	15.927399	-0.052487	3.963792
268.121639	5336.951426	15.932403	-0.052476	3.960949
268.170584	5328.974657	15.937408	-0.052479	3.958112
268.028046	5320.945377	15.942413	-0.052447	3.955251
268.145992	5312.932948	15.947418	-0.052464	3.952398
267.803442	5304.922504	15.952423	-0.052394	3.949536
267.784177	5296.950266	15.957427	-0.052385	3.946691
267.692998	5288.985587	15.962432	-0.052363	3.943846
267.429127	5280.981087	15.967437	-0.052308	3.940981
267.594571	5273.005728	15.972442	-0.052334	3.938132
267.590030	5264.928550	15.977447	-0.052327	3.935242
267.595505	5256.946582	15.982451	-0.052323	3.932384
267.689479	5248.941593	15.987456	-0.052335	3.929517
267.579053	5240.966643	15.992461	-0.052309	3.926655
267.790661	5232.983003	15.997466	-0.052343	3.923794
267.595999	5225.003149	16.002471	-0.052301	3.920924
267.583587	5217.019065	16.007475	-0.052294	3.918054
267.631466	5208.995240	16.012480	-0.052297	3.915169
267.261045	5200.953721	16.017485	-0.052223	3.912268
267.484565	5192.950083	16.022490	-0.052259	3.909389
267.622777	5184.978313	16.027495	-0.052279	3.906518
267.157922	5176.971016	16.032499	-0.052187	3.903621
267.436800	5168.989867	16.037504	-0.052234	3.900745
267.499292	5160.974851	16.042509	-0.052240	3.897851
267.500460	5152.973309	16.047514	-0.052235	3.894958
267.369162	5144.973489	16.052519	-0.052205	3.892061
267.222596	5136.942573	16.057523	-0.052172	3.889150
267.345628	5128.988684	16.062528	-0.052189	3.886271
267.287163	5120.973724	16.067533	-0.052173	3.883363
267.011077	5113.016004	16.072538	-0.052116	3.880470
267.149426	5105.005136	16.077543	-0.052136	3.877563
267.105158	5096.975717	16.082547	-0.052123	3.874644
267.136448	5088.736352	16.087552	-0.052123	3.871648
267.050566	5080.814948	16.092557	-0.052102	3.868763
266.895681	5072.907539	16.097562	-0.052067	3.865879
266.932991	5064.916834	16.102567	-0.052069	3.862967
266.681397	5056.937730	16.107571	-0.052017	3.860051
266.905008	5049.005283	16.112576	-0.052053	3.857160
266.812243	5040.969759	16.117581	-0.052030	3.854222
266.928222	5032.957855	16.122586	-0.052046	3.851295
266.983211	5024.975862	16.127591	-0.052051	3.848375
266.958342	5016.980506	16.132595	-0.052041	3.845447
266.843109	5009.046563	16.137600	-0.052014	3.842537
266.439038	5001.023455	16.142605	-0.051933	3.839586
266.691022	4993.046211	16.147610	-0.051975	3.836663
266.682434	4985.017478	16.152615	-0.051968	3.833713
266.549195	4976.988430	16.157619	-0.051937	3.830759
266.690767	4968.992395	16.162624	-0.051958	3.827820
266.557859	4960.996103	16.167629	-0.051928	3.824874
266.586092	4953.068786	16.172634	-0.051928	3.821953
266.467327	4945.058657	16.177639	-0.051900	3.818997
266.569218	4937.059803	16.182643	-0.051914	3.816047
266.184722	4929.080074	16.187648	-0.051837	3.813092
266.140240	4921.029518	16.192653	-0.051823	3.810116
266.169570	4913.080529	16.197658	-0.051823	3.807176
266.101837	4905.048934	16.202663	-0.051805	3.804201
266.032791	4897.092810	16.207667	-0.051787	3.801252
266.051126	4889.111656	16.212672	-0.051785	3.798293
265.801128	4881.110528	16.217677	-0.051733	3.795319
265.948666	4873.026659	16.222682	-0.051755	3.792320
265.908819	4865.036694	16.227687	-0.051742	3.789350
266.032857	4857.049946	16.232691	-0.051760	3.786382
266.014086	4849.093897	16.237696	-0.051751	3.783421
265.803162	4841.066835	16.242701	-0.051706	3.780426
265.938632	4833.114923	16.247706	-0.051726	3.777464
265.829880	4825.058498	16.252711	-0.051700	3.774456
265.660640	4817.075738	16.257715	-0.051663	3.771471
265.896453	4809.040488	16.262720	-0.051702	3.768474
265.749969	4801.075762	16.267725	-0.051669	3.765491
265.684410	4793.111627	16.272730	-0.051651	3.762509
265.695717	4785.064976	16.277735	-0.051648	3.759495
265.772059	4777.127324	16.282739	-0.051657	3.756521
265.691226	4769.073395	16.287744	-0.051636	3.753497
265.545675	4761.036662	16.292749	-0.051603	3.750476
265.901266	4753.061663	16.297754	-0.051664	3.747488
265.655972	4745.056526	16.302759	-0.051613	3.744471
265.369641	4737.136801	16.307763	-0.051554	3.741483
265.589593	4729.119669	16.312768	-0.051590	3.738468
265.457368	4721.122819	16.317773	-0.051560	3.735450
265.459408	4713.141383	16.322778	-0.051555	3.732439
265.321567	4705.095096	16.327783	-0.051524	3.729397
265.254689	4697.133505	16.332787	-0.051506	3.726387
265.294992	4689.170725	16.337792	-0.051508	3.723376
265.114316	4681.146891	16.342797	-0.051469	3.720334
265.295931	4673.192135	16.347802	-0.051497	3.717325
265.258391	4665.141795	16.352807	-0.051485	3.714271
265.012467	4657.047400	16.357811	-0.051433	3.711194
265.070125	4649.111099	16.362816	-0.051439	3.708181
265.111499	4641.082120	16.367821	-0.051441	3.705130
265.138716	4633.175514	16.372826	-0.051441	3.702123
264.827921	4625.179367	16.377831	-0.051377	3.699071
265.122086	4617.171632	16.382835	-0.051427	3.696027
265.109169	4609.189726	16.387840	-0.051419	3.692983
264.865668	4601.143753	16.392845	-0.051368	3.689906
264.983376	4593.191844	16.397850	-0.051384	3.686871
265.090615	4585.176931	16.402855	-0.051399	3.683810
264.844925	4577.217380	16.407859	-0.051348	3.680758
264.970740	4569.247117	16.412864	-0.051366	3.677709
264.837688	4561.202195	16.417869	-0.051336	3.674622
264.805615	4553.221600	16.422874	-0.051324	3.671560
264.811033	4545.188260	16.427879	-0.051320	3.668476
264.833396	4537.186528	16.432883	-0.051318	3.665402
264.876952	4529.252560	16.437888	-0.051321	3.662352
264.441882	4521.261156	16.442893	-0.051235	3.659265
264.524203	4513.247178	16.447898	-0.051244	3.656180
264.682533	4505.223418	16.452903	-0.051268	3.653091
264.350760	4497.195420	16.457907	-0.051201	3.649985
264.374269	4489.240548	16.462912	-0.051200	3.646913
264.280481	4481.257648	16.467917	-0.051177	3.643825
264.275935	4473.264115	16.472922	-0.051171	3.640733
264.137126	4465.292310	16.477927	-0.051140	3.637643
264.282478	4457.248847	16.482931	-0.051161	3.634530
264.189706	4449.237632	16.487936	-0.051139	3.631420
264.175048	4441.214210	16.492941	-0.051130	3.628306
264.098017	4433.234185	16.497946	-0.051111	3.625203
264.321396	4425.256013	16.502951	-0.051147	3.622107
264.103009	4417.280356	16.507955	-0.051101	3.618997
264.038117	4409.297628	16.512960	-0.051083	3.615886
264.091868	4401.272590	16.517965	-0.051088	3.612759
263.918407	4393.283391	16.522970	-0.051050	3.609637
263.842333	4385.314242	16.527975	-0.051030	3.606523
263.806402	4377.313225	16.532979	-0.051018	3.603395
263.968942	4369.336899	16.537984	-0.051043	3.600279
263.722321	4361.366454	16.542989	-0.050992	3.597152
263.721727	4353.374225	16.547994	-0.050986	3.594020
263.854780	4345.304548	16.552999	-0.051005	3.590858
263.616071	4337.364181	16.558003	-0.050956	3.587734
263.645381	4329.368534	16.563008	-0.050956	3.584594
263.720668	4321.395593	16.568013	-0.050964	3.581460
263.642399	4313.387666	16.573018	-0.050944	3.578306
263.504460	4305.384070	16.578023	-0.050913	3.575149
263.470614	4297.356246	16.583027	-0.050901	3.571983
263.738187	4289.371154	16.588032	-0.050946	3.568839
263.428866	4281.373039	16.593037	-0.050883	3.565671
263.716831	4273.415449	16.598042	-0.050931	3.562534
263.489054	4265.442974	16.603047	-0.050883	3.559372
263.550066	4257.446809	16.608051	-0.050889	3.556207
263.463134	4249.383726	16.613056	-0.050867	3.553008
263.246613	4241.309300	16.618061	-0.050821	3.549798
263.243868	4233.370100	16.623066	-0.050815	3.546645
263.256096	4225.374821	16.628071	-0.050812	3.543468
263.077284	4217.379895	16.633075	-0.050773	3.540282
263.315432	4209.425879	16.638080	-0.050812	3.537122
263.091238	4201.410444	16.643085	-0.050765	3.533920
262.997893	4193.405767	16.648090	-0.050742	3.530724
263.187002	4185.405696	16.653095	-0.050772	3.527536
262.923273	4177.420704	16.658099	-0.050718	3.524337
262.861509	4169.494766	16.663104	-0.050701	3.521164
262.794746	4161.470383	16.668109	-0.050683	3.517950
263.026942	4153.465481	16.673114	-0.050721	3.514749
263.053980	4145.467987	16.678119	-0.050720	3.511542
262.909749	4137.450577	16.683123	-0.050688	3.508319
262.961158	4129.451114	16.688128	-0.050692	3.505106
262.700863	4121.495533	16.693133	-0.050638	3.501898
262.650044	4113.526444	16.698138	-0.050623	3.498689
262.507343	4105.536228	16.703143	-0.050591	3.495464
262.594864	4097.526198	16.708147	-0.050602	3.492237
262.451520	4089.540061	16.713152	-0.050570	3.489008
262.423705	4081.533016	16.718157	-0.050559	3.485772
262.513560	4073.589756	16.723162	-0.050571	3.482562
262.644864	4065.578054	16.728167	-0.050590	3.479323
262.500605	4057.606319	16.733171	-0.050557	3.476088
262.633991	4049.568528	16.738176	-0.050577	3.472833
262.399503	4041.537455	16.743181	-0.050527	3.469565
262.247627	4033.578907	16.748186	-0.050494	3.466326
262.258055	4025.581161	16.753191	-0.050490	3.463074
262.307887	4017.575512	16.758195	-0.050494	3.459816
262.225375	4009.627056	16.763200	-0.050473	3.456575
262.212313	4001.574169	16.768205	-0.050465	3.453290
262.229819	3993.567769	16.773210	-0.050463	3.450022
262.086534	3985.632339	16.778215	-0.050431	3.446774
262.026437	3977.597021	16.783219	-0.050414	3.443485
262.036020	3969.653695	16.788224	-0.050411	3.440233
262.041550	3961.648156	16.793229	-0.050406	3.436953
261.879267	3953.654059	16.798234	-0.050371	3.433668
262.000410	3945.611085	16.803239	-0.050388	3.430370
261.917539	3937.622882	16.808243	-0.050367	3.427084
261.887459	3929.641842	16.813248	-0.050356	3.423799
261.751918	3921.664277	16.818253	-0.050325	3.420510
261.982195	3913.668815	16.823258	-0.050363	3.417222
261.756423	3905.714881	16.828263	-0.050315	3.413933
261.661584	3897.650573	16.833267	-0.050292	3.410599
261.992840	3889.712034	16.838272	-0.050348	3.407329
261.911768	3881.718776	16.843277	-0.050328	3.404018
261.627504	3873.777421	16.848282	-0.050269	3.400719
261.660782	3865.785730	16.853287	-0.050270	3.397407
261.624117	3857.740013	16.858291	-0.050258	3.394067
261.774361	3849.691035	16.863296	-0.050280	3.390729
261.488075	3841.713713	16.868301	-0.050222	3.387402
261.671234	3833.714473	16.873306	-0.050250	3.384079
261.533546	3825.774132	16.878311	-0.050219	3.380765
261.525752	3817.787976	16.883315	-0.050212	3.377435
261.614940	3809.788007	16.888320	-0.050223	3.374098
261.484436	3801.778790	16.893325	-0.050194	3.370747
261.257599	3793.822387	16.898330	-0.050146	3.367411
261.318576	3785.828477	16.903335	-0.050152	3.364066
261.233702	3777.836394	16.908339	-0.050131	3.360713
261.204498	3769.881759	16.913344	-0.050120	3.357375
261.212793	3761.857519	16.918349	-0.050116	3.354005
261.352603	3753.810685	16.923354	-0.050136	3.350627
261.379030	3745.845491	16.928359	-0.050136	3.347276
261.087230	3737.864019	16.933363	-0.050076	3.343904
261.129273	3729.897977	16.938368	-0.050079	3.340546
260.898295	3721.911970	16.943373	-0.050030	3.337167
260.990570	3713.898549	16.948378	-0.050042	3.333785
260.791324	3705.888489	16.953383	-0.049999	3.330389
260.797330	3697.896699	16.958387	-0.049995	3.327006
260.953524	3689.914562	16.963392	-0.050019	3.323629
260.660349	3681.929310	16.968397	-0.049959	3.320230
260.887979	3673.956355	16.973402	-0.049996	3.316853
260.807102	3665.967337	16.978407	-0.049975	3.313454
260.559984	3657.929444	16.983411	-0.049924	3.310024
260.688614	3649.963299	16.988416	-0.049942	3.306635
260.829913	3641.947789	16.993421	-0.049963	3.303223
260.967947	3633.974418	16.998426	-0.049983	3.299824
260.652592	3626.046109	17.003431	-0.049919	3.296425
260.637621	3618.014582	17.008435	-0.049911	3.292989
260.621798	3610.017032	17.013440	-0.049902	3.289563
260.408405	3602.059445	17.018445	-0.049857	3.286144
260.313221	3594.101035	17.023450	-0.049834	3.282726
260.570475	3586.032648	17.028455	-0.049877	3.279270
260.310825	3578.102217	17.033459	-0.049823	3.275850
260.209693	3570.114332	17.038464	-0.049798	3.272407
260.404962	3562.060861	17.043469	-0.049829	3.268945
260.167878	3554.075519	17.048474	-0.049780	3.265491
260.000815	3546.137147	17.053479	-0.049743	3.262056
260.037471	3538.145973	17.058483	-0.049745	3.258603
260.200110	3530.133666	17.063488	-0.049769	3.255143
260.078950	3522.134298	17.068493	-0.049741	3.251673
260.038603	3514.137523	17.073498	-0.049728	3.248203
260.080184	3506.138874	17.078503	-0.049731	3.244732
259.768071	3498.212377	17.083507	-0.049667	3.241275
260.024909	3490.218056	17.088512	-0.049710	3.237807
259.984318	3482.178861	17.093517	-0.049697	3.234305
259.924153	3474.133046	17.098522	-0.049680	3.230794
259.934401	3466.171652	17.103527	-0.049676	3.227320
259.765390	3458.168467	17.108531	-0.049639	3.223816
259.682156	3450.216679	17.113536	-0.049619	3.220334
259.629469	3442.264966	17.118541	-0.049603	3.216850
259.707760	3434.249781	17.123546	-0.049612	3.213340
259.713450	3426.235945	17.128551	-0.049608	3.209823
259.613436	3418.257926	17.133555	-0.049584	3.206314
259.497001	3410.315790	17.138560	-0.049557	3.202816
259.414520	3402.321058	17.143565	-0.049536	3.199293
259.441972	3394.339592	17.148570	-0.049536	3.195776
259.482821	3386.318250	17.153575	-0.049538	3.192238
259.324750	3378.310645	17.158579	-0.049503	3.188694
259.564088	3370.316347	17.163584	-0.049542	3.185168
259.420310	3362.349178	17.168589	-0.049510	3.181635
259.441189	3354.382163	17.173594	-0.049508	3.178104
259.231987	3346.417302	17.178599	-0.049464	3.174561
259.229583	3338.388118	17.183603	-0.049458	3.170994
259.221941	3330.426013	17.188608	-0.049451	3.167453
258.984024	3322.416617	17.193613	-0.049402	3.163877
259.173480	3314.437249	17.198618	-0.049431	3.160328
259.022278	3306.495665	17.203623	-0.049398	3.156778
259.026773	3298.434083	17.208627	-0.049393	3.153177
259.028803	3290.470556	17.213632	-0.049388	3.149615
258.952190	3282.453344	17.218637	-0.049368	3.146022
258.792860	3274.498681	17.223642	-0.049333	3.142449
258.742865	3266.518775	17.228647	-0.049319	3.138866
258.767323	3258.517077	17.233651	-0.049318	3.135272
258.604252	3250.553430	17.238656	-0.049282	3.131682
258.625841	3242.540578	17.243661	-0.049280	3.128075
258.778666	3234.532977	17.248666	-0.049303	3.124472
258.646250	3226.613277	17.253671	-0.049273	3.120891
258.384689	3218.637536	17.258675	-0.049219	3.117275
258.587591	3210.626347	17.263680	-0.049252	3.113660
258.424403	3202.598863	17.268685	-0.049216	3.110016
258.450654	3194.623875	17.273690	-0.049215	3.106401
258.477609	3186.657403	17.278695	-0.049215	3.102785
258.430454	3178.652035	17.283699	-0.049200	3.099145
258.594769	3170.677365	17.288704	-0.049226	3.095523
258.299764	3162.683536	17.293709	-0.049165	3.091868
258.426369	3154.674576	17.298714	-0.049183	3.088220
258.385767	3146.705577	17.303719	-0.049170	3.084579
258.342028	3138.749742	17.308723	-0.049157	3.080939
258.336616	3130.793993	17.313728	-0.049150	3.077297
258.135723	3122.745671	17.318733	-0.049107	3.073599
258.011374	3114.676908	17.323738	-0.049079	3.069891
258.256376	3106.710679	17.328743	-0.049119	3.066242
258.210400	3098.742849	17.333747	-0.049105	3.062575
258.261021	3090.796379	17.338752	-0.049109	3.058918
258.033335	3082.820269	17.343757	-0.049061	3.055230
258.013117	3074.828529	17.348762	-0.049052	3.051540
257.962390	3066.870539	17.353767	-0.049037	3.047859
257.765510	3058.880632	17.358771	-0.048995	3.044152
257.821714	3050.910764	17.363776	-0.049000	3.040463
257.794553	3042.949090	17.368781	-0.048990	3.036768
257.821458	3034.937097	17.373786	-0.048989	3.033048
257.901501	3026.915308	17.378791	-0.048999	3.029322
257.697027	3018.931639	17.383795	-0.048955	3.025595
257.544940	3011.003318	17.388800	-0.048921	3.021891
257.449273	3002.996006	17.393805	-0.048898	3.018149
257.540232	2994.999164	17.398810	-0.048910	3.014417
257.415490	2987.027476	17.403815	-0.048881	3.010680
257.378482	2979.027225	17.408819	-0.048869	3.006931
257.353447	2971.064317	17.413824	-0.048858	3.003194
257.264342	2963.090855	17.418829	-0.048836	2.999445
257.146423	2955.131120	17.423834	-0.048809	2.995696
257.181618	2947.085681	17.428839	-0.048810	2.991910
257.133764	2939.092972	17.433843	-0.048796	2.988139
257.137969	2931.099559	17.438848	-0.048791	2.984366
257.042873	2923.145970	17.443853	-0.048768	2.980602
257.152821	2915.165447	17.448858	-0.048783	2.976831
257.031513	2907.193350	17.453863	-0.048755	2.973048
256.973623	2899.178644	17.458867	-0.048739	2.969242
256.893367	2891.229187	17.463872	-0.048718	2.965462
256.826917	2883.257598	17.468877	-0.048701	2.961667
256.932670	2875.270526	17.473882	-0.048715	2.957868
256.803943	2867.307161	17.478887	-0.048685	2.954064
256.680293	2859.278433	17.483891	-0.048657	2.950224
256.756418	2851.297995	17.488896	-0.048666	2.946412
256.762604	2843.322391	17.493901	-0.048661	2.942595
256.726758	2835.349334	17.498906	-0.048649	2.938771
256.583793	2827.397025	17.503911	-0.048617	2.934946
256.572218	2819.360995	17.508915	-0.048610	2.931083
256.708255	2811.389471	17.513920	-0.048630	2.927254
256.658892	2803.408438	17.518925	-0.048615	2.923406
256.381010	2795.470086	17.523930	-0.048558	2.919561
256.358923	2787.503294	17.528935	-0.048548	2.915710
256.398111	2779.410034	17.533939	-0.048550	2.911797
256.492066	2771.410480	17.538944	-0.048562	2.907927
256.282305	2763.470466	17.543949	-0.048518	2.904064
256.527503	2755.485717	17.548954	-0.048558	2.900198
256.437313	2747.545402	17.553959	-0.048536	2.896331
256.204504	2739.558528	17.558963	-0.048487	2.892429
256.225666	2731.570340	17.563968	-0.048485	2.888534
256.378277	2723.556567	17.568973	-0.048508	2.884629
256.197014	2715.640546	17.573978	-0.048469	2.880748
256.162981	2707.673615	17.578983	-0.048457	2.876845
256.276210	2699.616419	17.583987	-0.048473	2.872900
256.269184	2691.658044	17.588992	-0.048466	2.868992
255.924543	2683.683691	17.593997	-0.048397	2.865052
255.964018	2675.733067	17.599002	-0.048399	2.861140
256.096065	2667.748702	17.604007	-0.048418	2.857210
255.798431	2659.787075	17.609011	-0.048357	2.853263
255.874047	2651.802650	17.614016	-0.048365	2.849319
255.746952	2643.792321	17.619021	-0.048336	2.845346
255.700019	2635.850863	17.624026	-0.048322	2.841406
255.468174	2627.903118	17.629031	-0.048274	2.837447
255.506402	2619.874366	17.634035	-0.048275	2.833458
255.653851	2611.860745	17.639040	-0.048297	2.829476
255.583712	2603.880037	17.644045	-0.048279	2.825493
255.653277	2595.932761	17.649050	-0.048286	2.821529
255.710074	2587.950655	17.654055	-0.048291	2.817542
255.515284	2579.977533	17.659059	-0.048250	2.813538
255.425896	2571.995041	17.664064	-0.048228	2.809530
255.511394	2564.001367	17.669069	-0.048238	2.805521
255.444877	2556.063902	17.674074	-0.048220	2.801526
255.278308	2548.126432	17.679079	-0.048184	2.797519
255.302139	2540.086834	17.684083	-0.048183	2.793466
255.352313	2532.103403	17.689088	-0.048187	2.789438
255.252232	2524.114380	17.694093	-0.048163	2.785391
255.226157	2516.156748	17.699098	-0.048152	2.781359
255.277078	2508.191861	17.704103	-0.048156	2.777322
254.942881	2500.220201	17.709107	-0.048089	2.773253
255.108663	2492.200768	17.714112	-0.048114	2.769183
254.881152	2484.242134	17.719117	-0.048066	2.765115
255.067029	2476.274994	17.724122	-0.048096	2.761061
255.070531	2468.324996	17.729127	-0.048091	2.756999
254.802555	2460.310741	17.734131	-0.048035	2.752881
255.097777	2452.255655	17.739136	-0.048085	2.748771
254.922503	2444.305058	17.744141	-0.048047	2.744680
254.723951	2436.381304	17.749146	-0.048005	2.740594
254.828940	2428.417776	17.754151	-0.048019	2.736501
254.785187	2420.413554	17.759155	-0.048005	2.732372
254.734582	2412.450667	17.764160	-0.047990	2.728257
254.762031	2404.455543	17.769165	-0.047990	2.724124
254.662708	2396.519569	17.774170	-0.047966	2.720008
254.657453	2388.563986	17.779175	-0.047960	2.715881
254.457065	2380.550749	17.784179	-0.047917	2.711705
254.395565	2372.594491	17.789184	-0.047900	2.707562
254.455364	2364.615541	17.794189	-0.047906	2.703408
254.402636	2356.645603	17.799194	-0.047890	2.699245
254.474936	2348.665184	17.804199	-0.047898	2.695078
254.281769	2340.684965	17.809203	-0.047857	2.690888
253.983747	2332.751957	17.814208	-0.047796	2.686709
253.857003	2324.791146	17.819213	-0.047767	2.682521
254.072609	2316.803158	17.824218	-0.047802	2.678333
254.083472	2308.823358	17.829223	-0.047798	2.674129
253.955129	2300.795556	17.834227	-0.047769	2.669885
254.038461	2292.836884	17.839232	-0.047779	2.665685
253.868101	2284.889801	17.844237	-0.047742	2.661467
253.967524	2276.892469	17.849242	-0.047755	2.657234
254.071615	2268.916063	17.854247	-0.047769	2.653005
254.079418	2260.920113	17.859251	-0.047765	2.648753
253.935879	2252.982202	17.864256	-0.047733	2.644515
253.762911	2245.039079	17.869261	-0.047695	2.640265
253.791249	2237.074152	17.874266	-0.047695	2.636011
253.750460	2229.098823	17.879271	-0.047682	2.631739
253.652624	2221.097250	17.884275	-0.047658	2.627442
253.692482	2213.141755	17.889280	-0.047660	2.623172
253.477299	2205.194226	17.894285	-0.047615	2.618883
253.573173	2197.215193	17.899290	-0.047627	2.614590
253.651357	2189.238107	17.904295	-0.047636	2.610290
253.603674	2181.248801	17.909299	-0.047622	2.605968
253.536923	2173.310580	17.914304	-0.047604	2.601665
253.494089	2165.343146	17.919309	-0.047591	2.597341
253.659460	2157.253892	17.924314	-0.047616	2.592957
253.593271	2149.200317	17.929319	-0.047598	2.588570
253.229080	2141.280187	17.934323	-0.047525	2.584228
253.548444	2133.340898	17.939328	-0.047579	2.579914
253.440266	2125.412271	17.944333	-0.047554	2.575570
253.149453	2117.478234	17.949338	-0.047494	2.571203
253.132279	2109.500032	17.954343	-0.047485	2.566823
252.954669	2101.558271	17.959347	-0.047447	2.562445
253.064536	2093.593538	17.964352	-0.047462	2.558066
253.063240	2085.629596	17.969357	-0.047456	2.553673
253.063167	2077.623035	17.974362	-0.047451	2.549248
252.853322	2069.684638	17.979367	-0.047406	2.544839
252.906777	2061.714236	17.984371	-0.047411	2.540423
252.905191	2053.773376	17.989376	-0.047405	2.536012
252.625321	2045.811784	17.994381	-0.047348	2.531561
252.617801	2037.837092	17.999386	-0.047341	2.527115
252.897277	2029.834659	18.004391	-0.047387	2.522666
252.803323	2021.884017	18.009395	-0.047364	2.518212
252.717269	2013.944532	18.014400	-0.047343	2.513756
252.566485	2005.943321	18.019405	-0.047310	2.509254
252.619876	1997.961319	18.024410	-0.047314	2.504768
252.557869	1990.037528	18.029415	-0.047297	2.500299
252.272471	1982.098219	18.034419	-0.047239	2.495797
252.375645	1974.099686	18.039424	-0.047252	2.491282
252.354077	1966.119084	18.044429	-0.047243	2.486759
252.254364	1958.182385	18.049434	-0.047219	2.482248
252.267970	1950.227340	18.054439	-0.047216	2.477726
252.266012	1942.235436	18.059443	-0.047210	2.473173
252.104057	1934.289757	18.064448	-0.047175	2.468627
251.999502	1926.321582	18.069453	-0.047150	2.464064
252.150660	1918.348683	18.074458	-0.047172	2.459508
252.073859	1910.422474	18.079463	-0.047153	2.454954
251.885164	1902.444302	18.084467	-0.047112	2.450354
251.884225	1894.490960	18.089472	-0.047107	2.445772
252.061070	1886.521837	18.094477	-0.047134	2.441187
251.901166	1878.573882	18.099482	-0.047099	2.436580
251.992330	1870.548171	18.104487	-0.047110	2.431938
251.825160	1862.572914	18.109491	-0.047074	2.427297
251.581636	1854.660927	18.114496	-0.047023	2.422677
251.578344	1846.698626	18.119501	-0.047017	2.418038
251.725789	1838.708625	18.124506	-0.047039	2.413386
251.686713	1830.745109	18.129511	-0.047026	2.408726
251.540877	1822.804839	18.134515	-0.046994	2.404061
251.672201	1814.862262	18.139520	-0.047013	2.399409
251.566564	1806.911473	18.144525	-0.046988	2.394723
251.408086	1798.930447	18.149530	-0.046953	2.390007
251.473242	1790.970202	18.154535	-0.046959	2.385311
251.286342	1783.040647	18.159539	-0.046919	2.380604
251.359229	1775.087291	18.164544	-0.046927	2.375894
251.144182	1767.122983	18.169549	-0.046882	2.371145
251.339815	1759.137829	18.174554	-0.046913	2.366407
251.245505	1751.221725	18.179559	-0.046890	2.361678
251.161984	1743.277022	18.184563	-0.046869	2.356923
251.091480	1735.303414	18.189568	-0.046850	2.352142
251.188212	1727.296394	18.194573	-0.046863	2.347344
250.850273	1719.383257	18.199578	-0.046795	2.342558
250.925150	1711.437978	18.204583	-0.046803	2.337777
250.843446	1703.460446	18.209587	-0.046783	2.332953
250.870487	1695.499346	18.214592	-0.046782	2.328139
250.779087	1687.537910	18.219597	-0.046760	2.323304
250.774376	1679.614117	18.224602	-0.046753	2.318489
250.860757	1671.660259	18.229607	-0.046764	2.313654
250.571069	1663.704155	18.234611	-0.046705	2.308775
250.515704	1655.761495	18.239616	-0.046689	2.303914
250.519523	1647.818082	18.244621	-0.046684	2.299047
250.576142	1639.849679	18.249626	-0.046689	2.294159
250.572878	1631.879082	18.254631	-0.046683	2.289255
250.648769	1623.905796	18.259635	-0.046692	2.284344
250.623664	1616.000373	18.264640	-0.046682	2.279457
250.198311	1608.106807	18.269645	-0.046597	2.274532
250.288148	1600.033935	18.274650	-0.046609	2.269529
250.217215	1592.093075	18.279655	-0.046590	2.264583
250.120854	1584.164122	18.284659	-0.046567	2.259632
250.098614	1576.226075	18.289664	-0.046557	2.254671
250.292542	1568.234075	18.294669	-0.046588	2.249684
250.090170	1560.308675	18.299674	-0.046545	2.244693
249.940560	1552.413501	18.304679	-0.046511	2.239714
249.942374	1544.451974	18.309683	-0.046506	2.234696
250.016630	1536.474236	18.314688	-0.046515	2.229662
249.954479	1528.516820	18.319693	-0.046498	2.224618
249.926958	1520.590557	18.324698	-0.046487	2.219585
250.193682	1512.623519	18.329703	-0.046531	2.214542
249.829297	1504.706257	18.334707	-0.046458	2.209462
249.770041	1496.767621	18.339712	-0.046442	2.204383
249.868572	1488.822849	18.344717	-0.046455	2.199304
249.872184	1480.886441	18.349722	-0.046450	2.194209
249.791590	1472.921236	18.354727	-0.046430	2.189077
249.493745	1464.982811	18.359731	-0.046369	2.183930
249.449863	1457.075262	18.364736	-0.046355	2.178813
249.411615	1449.122462	18.369741	-0.046343	2.173656
249.449926	1441.152451	18.374746	-0.046344	2.168483
249.251265	1433.244752	18.379751	-0.046302	2.163316
249.141366	1425.321435	18.384755	-0.046276	2.158134
249.198316	1417.363111	18.389760	-0.046281	2.152933
249.245161	1409.380000	18.394765	-0.046285	2.147701
249.123046	1401.458984	18.399770	-0.046256	2.142482
249.327934	1393.516594	18.404775	-0.046289	2.137267
249.114005	1385.577104	18.409779	-0.046244	2.132002
249.067268	1377.646980	18.414784	-0.046230	2.126745
249.160728	1369.706663	18.419789	-0.046242	2.121482
249.015830	1361.797607	18.424794	-0.046209	2.116204
249.137497	1353.784837	18.429799	-0.046227	2.110869
248.887767	1345.849633	18.434803	-0.046175	2.105537
248.956484	1337.927424	18.439808	-0.046182	2.100231
248.856233	1330.017193	18.444813	-0.046158	2.094903
248.759639	1322.072490	18.449818	-0.046135	2.089538
248.742439	1314.154005	18.454823	-0.046126	2.084185
248.515163	1306.248001	18.459827	-0.046078	2.078806
248.480990	1298.320934	18.464832	-0.046067	2.073418
248.585787	1290.345215	18.469837	-0.046081	2.067996
248.290596	1282.449206	18.474842	-0.046020	2.062575
248.448903	1274.514421	18.479847	-0.046044	2.057158
248.403343	1266.562354	18.484851	-0.046030	2.051694
248.428028	1258.615741	18.489856	-0.046030	2.046227
248.294931	1250.718468	18.494861	-0.045999	2.040763
248.401678	1242.784176	18.499866	-0.046014	2.035283
248.320089	1234.841587	18.504871	-0.045993	2.029764
248.277331	1226.904611	18.509875	-0.045980	2.024237
248.353792	1218.985574	18.514880	-0.045989	2.018720
248.086011	1211.095535	18.519885	-0.045934	2.013173
248.049605	1203.147854	18.524890	-0.045921	2.007593
248.055340	1195.233530	18.529895	-0.045917	2.002026
247.850422	1187.339304	18.534899	-0.045873	1.996436
247.991004	1179.371479	18.539904	-0.045894	1.990814
247.855643	1171.462462	18.544909	-0.045864	1.985189
247.955505	1163.534111	18.549914	-0.045877	1.979559
247.785126	1155.652351	18.554919	-0.045840	1.973917
247.825729	1147.686128	18.559923	-0.045842	1.968221
247.706022	1139.795769	18.564928	-0.045814	1.962546
247.695047	1131.895126	18.569933	-0.045807	1.956859
247.375775	1123.955677	18.574938	-0.045742	1.951094
247.773891	1115.956565	18.579943	-0.045811	1.945346
247.684733	1108.065570	18.584947	-0.045789	1.939607
247.572276	1100.169375	18.589952	-0.045762	1.933844
247.544114	1092.246518	18.594957	-0.045752	1.928054
247.553838	1084.323015	18.599962	-0.045748	1.922251
247.520123	1076.444600	18.604967	-0.045736	1.916457
247.113668	1068.548689	18.609971	-0.045655	1.910592
247.169286	1060.619156	18.614976	-0.045660	1.904736
247.165537	1052.719781	18.619981	-0.045654	1.898877
247.179118	1044.794564	18.624986	-0.045651	1.892983
247.056845	1036.896052	18.629991	-0.045623	1.887075
246.814873	1029.012251	18.634995	-0.045573	1.881146
246.812158	1021.116807	18.640000	-0.045567	1.875216
246.713430	1013.175511	18.645005	-0.045543	1.869222
246.893683	1005.235876	18.650010	-0.045571	1.863242
246.801506	997.361364	18.655015	-0.045549	1.857261
246.676658	989.450268	18.660019	-0.045520	1.851229
246.749332	981.527792	18.665024	-0.045528	1.845192
246.630033	973.662861	18.670029	-0.045501	1.839156
246.585271	965.752304	18.675034	-0.045487	1.833074
246.493379	957.856250	18.680039	-0.045464	1.826977
246.426303	949.951332	18.685043	-0.045446	1.820856
246.535874	942.063429	18.690048	-0.045462	1.814749
246.352060	934.165202	18.695053	-0.045422	1.808578
246.089779	926.305400	18.700058	-0.045368	1.802406
246.139575	918.414835	18.705063	-0.045372	1.796226
245.972174	910.460806	18.710067	-0.045335	1.789949
246.158736	902.537273	18.715072	-0.045364	1.783717
246.138487	894.659005	18.720077	-0.045355	1.777474
246.028714	886.767047	18.725082	-0.045329	1.771187
245.973795	878.899112	18.730087	-0.045314	1.764903
245.913735	871.025360	18.735091	-0.045297	1.758592
245.898822	863.141996	18.740096	-0.045289	1.752256
245.791403	855.251152	18.745101	-0.045264	1.745879
245.630774	847.390787	18.750106	-0.045228	1.739496
245.853048	839.488594	18.755111	-0.045264	1.733105
245.626306	831.609914	18.760115	-0.045217	1.726652
245.633560	823.740639	18.765120	-0.045213	1.720212
245.535693	815.890194	18.770125	-0.045189	1.713750
245.411801	807.989988	18.775130	-0.045161	1.707219
245.364371	800.123264	18.780135	-0.045147	1.700701
245.207484	792.263856	18.785139	-0.045112	1.694149
245.155642	784.377438	18.790144	-0.045097	1.687563
244.893991	776.539950	18.795149	-0.045043	1.680965
244.954561	768.654940	18.800154	-0.045049	1.674343
245.016680	760.769197	18.805159	-0.045055	1.667695
244.993774	752.893912	18.810163	-0.045045	1.661018
244.929900	745.047256	18.815168	-0.045028	1.654332
245.091227	737.147770	18.820173	-0.045053	1.647605
244.779877	729.332812	18.825178	-0.044990	1.640858
244.745719	721.483939	18.830183	-0.044978	1.634092
244.704204	713.558689	18.835187	-0.044965	1.627230
244.749715	705.702227	18.840192	-0.044968	1.620412
244.832021	697.842289	18.845197	-0.044978	1.613567
244.801161	689.979293	18.850202	-0.044967	1.606674
244.793461	682.145929	18.855207	-0.044960	1.599781
244.558921	674.331796	18.860211	-0.044911	1.592842
244.363889	666.498848	18.865216	-0.044869	1.585862
244.232426	658.677522	18.870221	-0.044839	1.578871
244.140127	650.830490	18.875226	-0.044817	1.571831
244.265316	642.963936	18.880231	-0.044835	1.564774
244.174995	635.143378	18.885235	-0.044813	1.557695
244.164973	627.296143	18.890240	-0.044805	1.550570
244.024408	619.462683	18.895245	-0.044774	1.543407
244.092398	611.617368	18.900250	-0.044781	1.536230
244.119297	603.782913	18.905255	-0.044781	1.529023
243.963274	595.968558	18.910259	-0.044747	1.521773
243.835208	588.175918	18.915264	-0.044717	1.514513
243.891322	580.321622	18.920269	-0.044722	1.507188
243.707485	572.527260	18.925274	-0.044683	1.499847
243.662054	564.718173	18.930279	-0.044669	1.492477
243.750509	556.867698	18.935283	-0.044680	1.485052
243.600346	549.097007	18.940288	-0.044647	1.477629
243.474009	541.259372	18.945293	-0.044618	1.470107
243.273558	533.458855	18.950298	-0.044575	1.462571
243.398505	525.639237	18.955303	-0.044593	1.455030
243.355450	517.820919	18.960307	-0.044580	1.447423
243.157598	510.063894	18.965312	-0.044538	1.439811
243.231944	502.262559	18.970317	-0.044546	1.432159
243.129765	494.465028	18.975322	-0.044522	1.424441
243.055131	486.702241	18.980327	-0.044503	1.416720
243.160977	478.875796	18.985331	-0.044517	1.408923
243.286786	471.079189	18.990336	-0.044535	1.401115
243.181492	463.329710	18.995341	-0.044510	1.393273
242.860801	455.571038	19.000346	-0.044445	1.385341
242.991806	447.787182	19.005351	-0.044465	1.377414
242.903356	440.015561	19.010355	-0.044443	1.369417
242.760643	432.272006	19.015360	-0.044411	1.361391
242.732732	424.520872	19.020365	-0.044400	1.353331
242.720628	416.744406	19.025370	-0.044393	1.345198
242.655398	409.011741	19.030375	-0.044375	1.337052
242.465756	401.274181	19.035379	-0.044335	1.328830
242.462685	393.529255	19.040384	-0.044329	1.320581
242.615512	385.719363	19.045389	-0.044352	1.312239
242.422415	377.928556	19.050394	-0.044311	1.303802
242.381732	370.218575	19.055399	-0.044298	1.295425
242.201491	362.508437	19.060403	-0.044259	1.286968
242.077417	354.821434	19.065408	-0.044231	1.278490
242.003875	347.109522	19.070413	-0.044212	1.269938
242.007922	339.393052	19.075418	-0.044207	1.261338
242.146939	331.673908	19.080423	-0.044228	1.252701
241.903600	324.001011	19.085427	-0.044177	1.243983
241.684955	316.349952	19.090432	-0.044132	1.235233
241.756434	308.619224	19.095437	-0.044140	1.226386
241.683018	300.946138	19.100442	-0.044121	1.217513
241.645911	293.269904	19.105447	-0.044109	1.208578
241.598257	285.597921	19.110451	-0.044094	1.199579
241.371969	277.971247	19.115456	-0.044047	1.190530
241.176335	270.332578	19.120461	-0.044005	1.181404
241.279175	262.653885	19.125466	-0.044019	1.172219
241.321871	255.002966	19.130471	-0.044022	1.162983
241.158228	247.382323	19.135475	-0.043986	1.153667
241.081898	239.729556	19.140480	-0.043967	1.144254
240.957357	232.123729	19.145485	-0.043939	1.134811
240.704096	224.527183	19.150490	-0.043886	1.125273
240.802104	216.915546	19.155495	-0.043899	1.115710
240.774081	209.301043	19.160499	-0.043889	1.106033
240.632115	201.748295	19.165504	-0.043857	1.096325
240.661153	194.152142	19.170509	-0.043857	1.086512
240.538473	186.602059	19.175514	-0.043829	1.076636
240.461466	179.034437	19.180519	-0.043810	1.066655
240.366021	171.491135	19.185523	-0.043787	1.056609
240.198180	163.969602	19.190528	-0.043751	1.046478
240.175534	156.443093	19.195533	-0.043741	1.036276
240.011614	148.939112	19.200538	-0.043706	1.025969
240.065947	141.428765	19.205543	-0.043711	1.015601
239.744338	133.970144	19.210547	-0.043646	1.005108
239.513344	126.527598	19.215552	-0.043598	0.994549
239.475003	119.016689	19.220557	-0.043585	0.983826
239.550564	111.534379	19.225562	-0.043594	0.973056
239.441448	104.106042	19.230567	-0.043569	0.962196
239.146502	96.720238	19.235571	-0.043509	0.951228
239.001679	89.325160	19.240576	-0.043477	0.940157
239.065815	81.907292	19.245581	-0.043484	0.928975
238.950415	74.545127	19.250586	-0.043457	0.917694
238.873273	67.180662	19.255591	-0.043438	0.906280
238.693336	60.087145	19.260595	-0.043399	0.895118