Fri Mar 12 11:24:02 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.952950	0.007647	0.000000	0.000012	0.717700
0.954013	0.012537	0.005005	0.000012	0.717710
0.896528	0.019011	0.010010	0.000023	0.717702
1.036109	-0.006930	0.015014	-0.000003	0.717699
1.025562	-0.000801	0.020019	-0.000001	0.717707
0.859180	0.024280	0.025024	0.000030	0.717698
1.024713	-0.000519	0.030029	-0.000000	0.717707
0.888626	0.022877	0.035034	0.000025	0.717705
0.778232	0.039803	0.040038	0.000046	0.717699
0.870060	0.028802	0.045043	0.000029	0.717709
0.990892	0.002134	0.050048	0.000007	0.717699
0.887620	0.024068	0.055053	0.000026	0.717705
0.919709	0.016720	0.060058	0.000020	0.717702
0.999657	0.000768	0.065062	0.000006	0.717698
1.094133	-0.011928	0.070067	-0.000012	0.717706
1.083790	-0.013534	0.075072	-0.000010	0.717699
0.925058	-0.101407	0.080077	0.000020	0.717469
0.893088	-0.141427	0.085082	0.000026	0.717378
0.888340	-0.140476	0.090086	0.000027	0.717378
1.104452	-0.174603	0.095091	-0.000013	0.717386
1.174109	-0.190300	0.100096	-0.000025	0.717379
1.153749	-0.182780	0.105101	-0.000021	0.717387
0.976243	-0.213680	0.110106	0.000012	0.717263
1.010881	-0.310286	0.115110	0.000006	0.717083
1.123116	-0.325597	0.120115	-0.000015	0.717092
0.934304	-0.297343	0.125120	0.000020	0.717081
0.809376	-0.269858	0.130125	0.000044	0.717091
0.988903	-0.370677	0.135130	0.000011	0.716955
0.960420	-0.464636	0.140134	0.000016	0.716758
0.902600	-0.451472	0.145139	0.000027	0.716763
1.016772	-0.476672	0.150144	0.000006	0.716753
0.799622	-0.464894	0.155149	0.000047	0.716700
0.920616	-0.612638	0.160154	0.000024	0.716450
0.912456	-0.612853	0.165158	0.000026	0.716446
0.842493	-0.595083	0.170163	0.000039	0.716456
0.856479	-0.671714	0.175168	0.000037	0.716309
0.818771	-0.750585	0.180173	0.000044	0.716139
0.958631	-0.777600	0.185178	0.000018	0.716134
0.892453	-0.769842	0.190182	0.000031	0.716126
0.881722	-0.885121	0.195187	0.000033	0.715894
0.906368	-0.891612	0.200192	0.000029	0.715889
0.999006	-0.906828	0.205197	0.000012	0.715891
0.954513	-1.062702	0.210202	0.000020	0.715566
0.962787	-1.071511	0.215206	0.000019	0.715551
0.966398	-1.083227	0.220211	0.000018	0.715529
0.988747	-1.236290	0.225216	0.000015	0.715233
0.744668	-1.189870	0.230221	0.000060	0.715238
0.923611	-1.283095	0.235226	0.000027	0.715116
0.689116	-1.346586	0.240230	0.000071	0.714907
0.679281	-1.341622	0.245235	0.000073	0.714913
0.741960	-1.469779	0.250240	0.000062	0.714680
0.922336	-1.534359	0.255245	0.000028	0.714616
0.636842	-1.530483	0.260250	0.000082	0.714522
0.600295	-1.648128	0.265254	0.000089	0.714275
0.891484	-1.696246	0.270259	0.000035	0.714282
0.917133	-1.845042	0.275264	0.000030	0.713995
0.869070	-1.846507	0.280269	0.000039	0.713975
0.741525	-1.932767	0.285274	0.000063	0.713758
0.868668	-2.009533	0.290278	0.000040	0.713650
0.791767	-2.068542	0.295283	0.000055	0.713505
0.620885	-2.112596	0.300288	0.000087	0.713357
0.597265	-2.172788	0.305293	0.000091	0.713228
0.721659	-2.296488	0.310298	0.000068	0.713026
0.275481	-2.269125	0.315302	0.000152	0.712922
0.338360	-2.384212	0.320307	0.000140	0.712714
0.011913	-2.365614	0.325312	0.000201	0.712635
-0.488525	-2.400114	0.330317	0.000294	0.712389
-2.555182	-2.032747	0.335322	0.000679	0.712387
-2.407842	-2.159272	0.340326	0.000652	0.712186
-2.826597	-2.130890	0.345331	0.000730	0.712094
-3.225996	-2.063808	0.350336	0.000805	0.712085
-3.150893	-2.151613	0.355341	0.000791	0.711937
-4.231754	-2.046850	0.360346	0.000992	0.711761
-4.064697	-2.077608	0.365350	0.000961	0.711759
-3.973681	-2.089767	0.370355	0.000945	0.711767
-4.728055	-2.084210	0.375360	0.001085	0.711509
-4.877014	-2.083702	0.380365	0.001113	0.711457
-4.785037	-2.101669	0.385370	0.001096	0.711454
-5.103253	-2.046268	0.390374	0.001156	0.711451
-4.851867	-2.199569	0.395379	0.001109	0.711234
-5.958140	-2.052045	0.400384	0.001315	0.711134
-5.661517	-2.102215	0.405389	0.001260	0.711139
-5.664710	-2.102166	0.410394	0.001261	0.711138
-5.797939	-2.137453	0.415398	0.001286	0.711020
-6.350562	-2.109880	0.420403	0.001389	0.710878
-6.549615	-2.078643	0.425408	0.001426	0.710869
-6.501657	-2.083682	0.430413	0.001418	0.710876
-6.455579	-2.093468	0.435418	0.001409	0.710872
-6.765186	-2.179265	0.440422	0.001467	0.710590
-7.498659	-2.074986	0.445427	0.001604	0.710537
-7.523684	-2.074172	0.450432	0.001609	0.710530
-7.459998	-2.080961	0.455437	0.001597	0.710538
-7.613055	-2.054986	0.460442	0.001626	0.710535
-7.492383	-2.184772	0.465446	0.001604	0.710319
-8.201119	-2.108403	0.470451	0.001736	0.710219
-8.600030	-2.039277	0.475456	0.001810	0.710214
-8.098632	-2.126807	0.480461	0.001717	0.710218
-8.420706	-2.068289	0.485466	0.001777	0.710219
-8.574740	-2.054013	0.490470	0.001806	0.710193
-8.869432	-2.149272	0.495475	0.001861	0.709897
-9.122035	-2.108678	0.500480	0.001908	0.709888
-9.641702	-2.011120	0.505485	0.002005	0.709897
-9.467939	-2.042644	0.510490	0.001973	0.709896
-9.417010	-2.054660	0.515494	0.001964	0.709890
-9.336015	-2.065944	0.520499	0.001949	0.709895
-9.813731	-2.108109	0.525504	0.002038	0.709641
-10.106049	-2.078971	0.530509	0.002093	0.709594
-9.860026	-2.122398	0.535514	0.002047	0.709595
-10.221189	-2.060815	0.540518	0.002115	0.709589
-10.203558	-2.058934	0.545523	0.002111	0.709598
-10.267197	-2.053262	0.550528	0.002123	0.709587
-10.104570	-2.179685	0.555533	0.002093	0.709392
-11.525666	-1.989700	0.560538	0.002358	0.709265
-11.413369	-2.012533	0.565542	0.002337	0.709259
-10.934970	-2.094217	0.570547	0.002249	0.709265
-11.524183	-1.993235	0.575552	0.002358	0.709257
-11.053721	-2.073387	0.580557	0.002271	0.709264
-10.893422	-2.100797	0.585562	0.002241	0.709266
-11.564862	-2.100009	0.590566	0.002367	0.709028
-12.002040	-2.056921	0.595571	0.002448	0.708957
-11.684157	-2.116589	0.600576	0.002389	0.708951
-11.776700	-2.097650	0.605581	0.002407	0.708956
-11.960618	-2.062271	0.610586	0.002441	0.708960
-12.099710	-2.040260	0.615590	0.002467	0.708954
-11.706444	-2.138548	0.620595	0.002394	0.708898
-12.867656	-2.063534	0.625600	0.002611	0.708633
-12.800068	-2.071655	0.630605	0.002598	0.708641
-13.072121	-2.024230	0.635610	0.002649	0.708638
-13.048058	-2.031530	0.640614	0.002645	0.708632
-12.836993	-2.063860	0.645619	0.002606	0.708642
-12.954050	-2.047879	0.650624	0.002628	0.708632
-12.859504	-2.087069	0.655629	0.002610	0.708587
-13.552450	-2.082478	0.660634	0.002739	0.708348
-13.653927	-2.067168	0.665638	0.002759	0.708342
-13.779873	-2.038850	0.670643	0.002782	0.708354
-14.091833	-1.989219	0.675648	0.002840	0.708341
-13.904852	-2.019089	0.680653	0.002806	0.708348
-13.540891	-2.082918	0.685658	0.002738	0.708349
-13.801301	-2.074063	0.690662	0.002787	0.708274
-14.636440	-2.053959	0.695667	0.002943	0.708015
-14.713223	-2.043049	0.700672	0.002957	0.708009
-14.893529	-2.009521	0.705677	0.002991	0.708012
-14.847820	-2.016666	0.710682	0.002983	0.708014
-14.937818	-2.003556	0.715686	0.002999	0.708007
-14.607979	-2.058424	0.720691	0.002938	0.708015
-15.202560	-1.956352	0.725696	0.003049	0.708007
-15.180750	-2.053596	0.730701	0.003045	0.707819
-16.011520	-1.963440	0.735706	0.003200	0.707702
-16.023155	-1.964451	0.740710	0.003202	0.707696
-15.735139	-2.012607	0.745715	0.003149	0.707702
-16.055922	-1.959955	0.750720	0.003209	0.707693
-15.511008	-2.053123	0.755725	0.003108	0.707700
-15.631490	-2.031892	0.760730	0.003130	0.707699
-15.810754	-2.002286	0.765734	0.003164	0.707694
-16.003119	-2.124680	0.770739	0.003200	0.707379
-16.779315	-1.990422	0.775744	0.003345	0.707371
-17.045176	-1.939855	0.780749	0.003394	0.707377
-16.302812	-2.070127	0.785754	0.003256	0.707381
-16.747514	-1.995811	0.790758	0.003339	0.707370
-16.861446	-1.971936	0.795763	0.003361	0.707377
-16.650371	-2.011553	0.800768	0.003322	0.707373
-16.709015	-2.101680	0.805773	0.003333	0.707171
-17.542216	-1.997110	0.810778	0.003488	0.707082
-17.570408	-1.996294	0.815782	0.003493	0.707073
-17.074945	-2.079722	0.820787	0.003401	0.707083
-17.746041	-1.964698	0.825792	0.003527	0.707073
-17.665136	-1.977380	0.830797	0.003512	0.707076
-17.429879	-2.018159	0.835802	0.003468	0.707078
-17.879111	-2.056731	0.840806	0.003552	0.706839
-18.561718	-1.977425	0.845811	0.003679	0.706754
-18.018750	-2.075698	0.850816	0.003578	0.706751
-18.078977	-2.064584	0.855821	0.003590	0.706751
-18.532019	-1.982750	0.860826	0.003674	0.706753
-18.442715	-2.001555	0.865830	0.003658	0.706747
-17.953283	-2.083406	0.870835	0.003567	0.706757
-18.801127	-2.076698	0.875840	0.003725	0.706467
-19.609353	-1.944523	0.880845	0.003876	0.706442
-19.312128	-1.995535	0.885850	0.003820	0.706446
-19.407326	-1.982421	0.890854	0.003838	0.706438
-19.226260	-2.009541	0.895859	0.003805	0.706448
-19.421484	-1.978558	0.900864	0.003841	0.706440
-19.013628	-2.048591	0.905869	0.003766	0.706445
-19.286935	-2.097557	0.910874	0.003817	0.706248
-20.425891	-1.958098	0.915878	0.004029	0.706120
-19.849585	-2.055754	0.920883	0.003922	0.706130
-19.946964	-2.042871	0.925888	0.003940	0.706120
-20.474939	-1.946318	0.930893	0.004039	0.706125
-20.010976	-2.027986	0.935898	0.003953	0.706127
-20.128365	-2.009788	0.940902	0.003975	0.706121
-20.368519	-2.055533	0.945907	0.004020	0.705942
-20.971973	-1.991593	0.950912	0.004132	0.705854
-20.647356	-2.045745	0.955917	0.004072	0.705861
-20.521284	-2.066211	0.960922	0.004049	0.705865
-21.173947	-1.954687	0.965926	0.004170	0.705855
-20.662846	-2.040103	0.970931	0.004075	0.705866
-20.826302	-2.034920	0.975936	0.004106	0.705817
-21.804708	-2.007983	0.980941	0.004288	0.705520
-21.703317	-2.023973	0.985946	0.004270	0.705524
-22.105806	-1.955296	0.990950	0.004345	0.705518
-21.838443	-1.998973	0.995955	0.004295	0.705525
-22.126280	-1.951666	1.000960	0.004349	0.705517
-21.901212	-1.990170	1.005965	0.004307	0.705520
-21.734781	-2.018220	1.010970	0.004276	0.705523
-22.484249	-2.021249	1.015974	0.004416	0.705247
-22.646271	-2.010404	1.020979	0.004446	0.705211
-22.879346	-1.972585	1.025984	0.004490	0.705203
-22.817809	-1.981162	1.030989	0.004479	0.705207
-22.700957	-2.000878	1.035994	0.004457	0.705209
-22.721899	-1.999288	1.040998	0.004461	0.705204
-22.672692	-2.004813	1.046003	0.004452	0.705211
-23.340695	-2.002610	1.051008	0.004577	0.704975
-23.856897	-1.956751	1.056013	0.004673	0.704881
-23.305535	-2.053582	1.061018	0.004571	0.704884
-23.788008	-1.972733	1.066022	0.004661	0.704873
-23.583364	-2.001553	1.071027	0.004623	0.704888
-23.512478	-2.018230	1.076032	0.004610	0.704880
-23.545823	-2.010397	1.081037	0.004616	0.704883
-23.613101	-2.100975	1.086042	0.004629	0.704676
-24.373916	-2.011523	1.091046	0.004771	0.704583
-24.255112	-2.029653	1.096051	0.004749	0.704589
-24.413348	-2.004822	1.101056	0.004779	0.704581
-24.498450	-1.987917	1.106061	0.004795	0.704585
-24.139490	-2.051689	1.111066	0.004728	0.704585
-24.660413	-1.972464	1.116070	0.004825	0.704557
-24.952693	-2.067559	1.121075	0.004880	0.704260
-25.252306	-2.017288	1.126080	0.004936	0.704253
-25.768338	-1.923633	1.131085	0.005032	0.704256
-25.330345	-2.000220	1.136090	0.004951	0.704259
-25.294289	-2.009639	1.141094	0.004944	0.704252
-25.301480	-2.004030	1.146099	0.004946	0.704261
-25.454345	-1.978723	1.151104	0.004974	0.704256
-26.199370	-1.994464	1.156109	0.005113	0.703956
-25.808815	-2.064685	1.161114	0.005041	0.703955
-26.513102	-1.944663	1.166118	0.005172	0.703943
-26.048782	-2.022618	1.171123	0.005086	0.703953
-26.075456	-2.023096	1.176128	0.005091	0.703942
-26.517011	-1.941363	1.181133	0.005173	0.703947
-26.015735	-2.028422	1.186138	0.005080	0.703952
-26.775309	-2.049972	1.191142	0.005222	0.703635
-27.035263	-2.002976	1.196147	0.005270	0.703636
-27.376282	-1.944583	1.201152	0.005334	0.703630
-26.982580	-2.015482	1.206157	0.005261	0.703629
-26.775547	-2.048497	1.211162	0.005223	0.703636
-27.371642	-1.947102	1.216166	0.005334	0.703626
-27.217983	-1.968396	1.221171	0.005305	0.703638
-27.409949	-2.069224	1.226176	0.005341	0.703365
-28.134685	-1.952660	1.231181	0.005476	0.703339
-27.965032	-1.980444	1.236186	0.005445	0.703343
-27.964568	-1.986644	1.241190	0.005445	0.703331
-27.780495	-2.013867	1.246195	0.005411	0.703342
-28.006386	-1.974838	1.251200	0.005453	0.703339
-27.919777	-1.997442	1.256205	0.005437	0.703324
-28.299409	-2.086698	1.261210	0.005508	0.703007
-28.941832	-1.977149	1.266214	0.005628	0.702996
-28.925168	-1.975608	1.271219	0.005625	0.703005
-28.553756	-2.045472	1.276224	0.005556	0.702997
-29.043119	-1.958190	1.281229	0.005648	0.702997
-28.917340	-1.977998	1.286234	0.005624	0.703002
-28.980922	-1.969800	1.291238	0.005636	0.702995
-29.209358	-2.078480	1.296243	0.005679	0.702693
-29.593395	-2.012448	1.301248	0.005751	0.702688
-29.880957	-1.962845	1.306253	0.005804	0.702684
-29.431204	-2.039725	1.311258	0.005721	0.702690
-29.756751	-1.985358	1.316262	0.005782	0.702682
-29.786177	-1.975485	1.321267	0.005787	0.702691
-29.422736	-2.077878	1.326272	0.005720	0.702615
-30.515392	-2.008712	1.331277	0.005924	0.702361
-30.488935	-2.009617	1.336282	0.005919	0.702368
-30.925823	-1.935393	1.341286	0.006000	0.702360
-30.401351	-2.024673	1.346291	0.005903	0.702368
-30.590234	-1.992779	1.351296	0.005938	0.702364
-30.856745	-1.946541	1.356301	0.005988	0.702361
-30.388031	-2.053173	1.361306	0.005901	0.702314
-31.348941	-2.006859	1.366310	0.006080	0.702061
-31.207913	-2.028079	1.371315	0.006054	0.702069
-31.335747	-2.006914	1.376320	0.006078	0.702065
-31.327770	-2.008616	1.381325	0.006077	0.702064
-31.339170	-2.002039	1.386330	0.006079	0.702073
-31.372485	-2.001741	1.391334	0.006086	0.702061
-31.215231	-2.107849	1.396339	0.006056	0.701903
-32.705644	-1.925652	1.401344	0.006334	0.701734
-32.569231	-1.949291	1.406349	0.006309	0.701735
-32.059979	-2.037176	1.411354	0.006214	0.701740
-32.257324	-2.005390	1.416358	0.006251	0.701733
-32.187306	-2.012715	1.421363	0.006238	0.701743
-32.274111	-1.998788	1.426368	0.006255	0.701739
-32.186683	-2.094220	1.431373	0.006239	0.701577
-33.087223	-2.002975	1.436378	0.006407	0.701437
-33.305208	-1.969857	1.441382	0.006447	0.701425
-33.202164	-1.982689	1.446387	0.006428	0.701436
-33.125342	-1.998209	1.451392	0.006414	0.701431
-33.173011	-1.989370	1.456397	0.006423	0.701432
-32.943918	-2.029112	1.461402	0.006381	0.701434
-33.196092	-2.089582	1.466406	0.006428	0.701220
-34.381334	-1.927720	1.471411	0.006649	0.701119
-33.987492	-1.998576	1.476416	0.006576	0.701118
-33.844047	-2.024434	1.481421	0.006549	0.701117
-34.035214	-1.986692	1.486426	0.006585	0.701124
-34.308922	-1.942401	1.491430	0.006636	0.701114
-33.836962	-2.021292	1.496435	0.006548	0.701124
-34.115558	-2.051226	1.501440	0.006601	0.700963
-35.161531	-1.912443	1.506445	0.006795	0.700866
-34.685044	-1.993145	1.511450	0.006707	0.700874
-34.729435	-1.989167	1.516454	0.006715	0.700866
-34.783751	-1.975022	1.521459	0.006726	0.700874
-34.675769	-1.996212	1.526464	0.006706	0.700870
-34.837044	-1.967770	1.531469	0.006736	0.700869
-34.939355	-2.101696	1.536474	0.006755	0.700560
-35.566366	-2.007255	1.541478	0.006872	0.700525
-35.300886	-2.049101	1.546483	0.006823	0.700535
-35.427615	-2.027241	1.551488	0.006847	0.700534
-35.538521	-2.008665	1.556493	0.006868	0.700531
-35.342512	-2.041511	1.561498	0.006831	0.700535
-35.602117	-2.115598	1.566502	0.006880	0.700290
-36.536375	-1.983943	1.571507	0.007054	0.700219
-36.772722	-1.943997	1.576512	0.007098	0.700214
-36.122313	-2.061650	1.581517	0.006977	0.700210
-36.207501	-2.042618	1.586522	0.006993	0.700218
-36.931800	-1.918270	1.591526	0.007128	0.700208
-36.358775	-2.016927	1.596531	0.007022	0.700214
-37.005546	-2.059262	1.601536	0.007142	0.699894
-37.689032	-1.940918	1.606541	0.007270	0.699887
-37.494383	-1.974332	1.611546	0.007234	0.699889
-37.237772	-2.023296	1.616550	0.007186	0.699882
-37.415211	-1.985699	1.621555	0.007219	0.699894
-37.531045	-1.968473	1.626560	0.007241	0.699886
-37.186804	-2.029603	1.631565	0.007177	0.699886
-37.400518	-2.112640	1.636570	0.007217	0.699640
-38.714106	-1.904835	1.641574	0.007462	0.699586
-38.225944	-1.988596	1.646579	0.007371	0.699592
-37.915016	-2.043671	1.651584	0.007314	0.699593
-38.520416	-1.935481	1.656589	0.007427	0.699593
-38.185127	-1.991325	1.661594	0.007364	0.699601
-37.890033	-2.054803	1.666598	0.007310	0.699578
-38.725049	-2.060375	1.671603	0.007465	0.699264
-39.322822	-1.954926	1.676608	0.007577	0.699261
-39.242966	-1.968177	1.681613	0.007562	0.699263
-38.529350	-2.092496	1.686618	0.007430	0.699269
-39.135511	-1.989241	1.691622	0.007543	0.699258
-39.071485	-1.996863	1.696627	0.007531	0.699266
-38.771186	-2.098999	1.701632	0.007475	0.699167
-40.153989	-1.960839	1.706637	0.007733	0.698946
-39.774781	-2.023447	1.711642	0.007662	0.698956
-39.780326	-2.025347	1.716646	0.007664	0.698950
-39.787854	-2.019864	1.721651	0.007665	0.698958
-39.971858	-1.988976	1.726656	0.007700	0.698953
-39.951151	-1.994789	1.731661	0.007696	0.698949
-39.842460	-2.092954	1.736666	0.007676	0.698788
-41.200096	-1.927581	1.741670	0.007929	0.698632
-40.791663	-1.996326	1.746675	0.007853	0.698640
-40.455865	-2.057261	1.751680	0.007791	0.698637
-41.218529	-1.922244	1.756685	0.007933	0.698635
-40.881958	-1.975830	1.761690	0.007870	0.698648
-40.886633	-1.980955	1.766694	0.007871	0.698635
-40.848980	-2.041654	1.771699	0.007865	0.698525
-41.760340	-1.966280	1.776704	0.008034	0.698347
-41.355629	-2.039891	1.781709	0.007959	0.698344
-41.435033	-2.021170	1.786714	0.007974	0.698353
-41.902045	-1.943333	1.791718	0.008061	0.698341
-41.523295	-2.006211	1.796723	0.007991	0.698351
-41.279958	-2.050195	1.801728	0.007946	0.698349
-41.852595	-2.080863	1.806733	0.008053	0.698078
-42.497794	-1.997785	1.811738	0.008173	0.698013
-42.488750	-2.002244	1.816742	0.008172	0.698007
-42.173093	-2.053605	1.821747	0.008113	0.698016
-42.524325	-1.993383	1.826752	0.008179	0.698011
-42.796604	-1.945748	1.831757	0.008230	0.698009
-42.221453	-2.047764	1.836762	0.008123	0.698010
-43.305334	-2.010179	1.841766	0.008325	0.697692
-43.378323	-1.994062	1.846771	0.008338	0.697698
-43.469393	-1.978785	1.851776	0.008356	0.697696
-43.429601	-1.986082	1.856781	0.008348	0.697695
-43.453631	-1.977739	1.861786	0.008353	0.697703
-43.559413	-1.962062	1.866790	0.008373	0.697696
-43.198732	-2.023526	1.871795	0.008306	0.697702
-43.870859	-2.040492	1.876800	0.008431	0.697423
-44.615432	-1.933865	1.881805	0.008570	0.697369
-44.277740	-1.989776	1.886810	0.008507	0.697377
-44.456897	-1.962503	1.891814	0.008541	0.697367
-44.467792	-1.958996	1.896819	0.008543	0.697370
-44.137133	-2.018634	1.901824	0.008482	0.697369
-44.211991	-2.005749	1.906829	0.008496	0.697367
-44.506127	-2.041914	1.911834	0.008551	0.697186
-45.436707	-1.933736	1.916838	0.008724	0.697068
-44.919156	-2.021694	1.921843	0.008628	0.697077
-45.271980	-1.959572	1.926848	0.008694	0.697075
-45.342615	-1.947976	1.931853	0.008707	0.697072
-44.769746	-2.047256	1.936858	0.008601	0.697078
-45.234785	-1.967952	1.941862	0.008688	0.697070
-45.617124	-2.013653	1.946867	0.008759	0.696837
-46.036604	-1.982980	1.951872	0.008837	0.696747
-46.047431	-1.981860	1.956877	0.008840	0.696745
-45.778814	-2.025533	1.961882	0.008790	0.696753
-46.108986	-1.971967	1.966886	0.008852	0.696742
-45.714821	-2.039566	1.971891	0.008778	0.696747
-45.971810	-1.993082	1.976896	0.008826	0.696748
-46.769482	-1.994451	1.981901	0.008975	0.696455
-46.698302	-2.013738	1.986906	0.008962	0.696441
-46.904870	-1.978926	1.991910	0.009001	0.696436
-46.852881	-1.986829	1.996915	0.008991	0.696439
-46.843306	-1.990646	2.001920	0.008990	0.696434
-46.788204	-2.009379	2.011917	0.008980	0.696415
-47.441879	-2.036361	2.021914	0.009102	0.696122
-47.806069	-1.970607	2.031910	0.009170	0.696122
-47.794907	-1.973915	2.041907	0.009168	0.696119
-47.604219	-2.005917	2.051904	0.009133	0.696122
-47.791212	-1.972039	2.061901	0.009168	0.696123
-47.614804	-2.003255	2.071898	0.009136	0.696122
-47.526552	-1.933944	2.081894	0.009120	0.696295
-46.836791	-1.988040	2.091891	0.008992	0.696435
-46.795939	-1.993848	2.101888	0.008985	0.696437
-46.774233	-1.997046	2.111885	0.008981	0.696438
-46.802877	-1.991301	2.121882	0.008987	0.696439
-46.886751	-1.974708	2.131878	0.009003	0.696441
-46.952236	-1.963808	2.141875	0.009015	0.696439
-46.773586	-1.996534	2.151872	0.008982	0.696436
-46.395752	-1.978455	2.161869	0.008912	0.696610
-45.726107	-2.029885	2.171866	0.008788	0.696748
-46.246398	-1.935330	2.181862	0.008885	0.696751
-45.715717	-2.031425	2.191859	0.008787	0.696747
-46.116880	-1.954555	2.201856	0.008862	0.696757
-45.366890	-1.930301	2.211853	0.008723	0.697078
-44.889196	-2.015677	2.221850	0.008634	0.697077
-45.084498	-1.979936	2.231846	0.008671	0.697078
-44.967314	-2.001737	2.241843	0.008650	0.697076
-44.303179	-1.983423	2.251840	0.008526	0.697354
-43.947257	-2.037754	2.261837	0.008460	0.697372
-44.144200	-2.001567	2.271834	0.008497	0.697373
-44.144693	-2.000805	2.281830	0.008498	0.697374
-43.294025	-2.000728	2.291827	0.008340	0.697682
-43.463112	-1.964059	2.301824	0.008372	0.697695
-43.296460	-1.992111	2.311821	0.008341	0.697697
-43.059944	-1.996231	2.321818	0.008297	0.697774
-42.579403	-1.965647	2.331814	0.008208	0.698010
-42.454980	-1.989123	2.341811	0.008186	0.698006
-42.759587	-1.933619	2.351808	0.008243	0.698008
-41.658530	-1.989578	2.361805	0.008038	0.698293
-41.818885	-1.933060	2.371802	0.008068	0.698349
-41.605048	-1.972408	2.381798	0.008029	0.698346
-41.462962	-1.955419	2.391795	0.008003	0.698431
-40.759702	-1.980279	2.401792	0.007872	0.698635
-40.462490	-2.033804	2.411789	0.007817	0.698633
-40.707396	-1.986989	2.421786	0.007863	0.698639
-40.187482	-1.978538	2.431782	0.007767	0.698844
-39.983850	-1.961495	2.441779	0.007729	0.698951
-40.148183	-1.930204	2.451776	0.007760	0.698955
-39.602095	-1.985691	2.461773	0.007659	0.699039
-39.049964	-1.973034	2.471770	0.007557	0.699264
-38.960787	-1.987955	2.481766	0.007540	0.699265
-38.957412	-1.990691	2.491763	0.007540	0.699260
-38.449222	-1.949143	2.501760	0.007446	0.699528
-37.928985	-2.008681	2.511757	0.007349	0.699595
-37.973160	-2.000512	2.521754	0.007358	0.699594
-38.073497	-1.958921	2.531750	0.007377	0.699642
-37.270528	-1.980496	2.541747	0.007228	0.699888
-37.382403	-1.958906	2.551744	0.007249	0.699891
-37.220878	-1.987229	2.561741	0.007219	0.699891
-36.584698	-1.982518	2.571738	0.007101	0.700130
-36.412682	-1.970983	2.581734	0.007070	0.700215
-36.254144	-2.000314	2.591731	0.007041	0.700212
-36.486336	-1.922856	2.601728	0.007084	0.700284
-35.243602	-2.023233	2.611725	0.006853	0.700529
-35.570433	-1.964505	2.621722	0.006914	0.700529
-35.448692	-1.986156	2.631718	0.006892	0.700529
-34.941818	-1.947163	2.641715	0.006798	0.700790
-34.598990	-1.968244	2.651712	0.006735	0.700871
-34.572246	-1.973841	2.661709	0.006730	0.700868
-34.453275	-1.964796	2.671706	0.006708	0.700929
-33.909616	-1.969171	2.681702	0.006607	0.701116
-33.957419	-1.960550	2.691699	0.006617	0.701115
-33.923449	-1.965777	2.701696	0.006611	0.701116
-32.930290	-1.991880	2.711693	0.006426	0.701421
-32.918097	-1.988128	2.721690	0.006424	0.701432
-32.745511	-2.018690	2.731686	0.006393	0.701432
-32.790418	-1.947734	2.741683	0.006401	0.701559
-31.858371	-2.025638	2.751680	0.006228	0.701737
-31.984138	-1.999485	2.761677	0.006252	0.701743
-32.005819	-1.995328	2.771674	0.006256	0.701743
-31.180144	-2.002507	2.781670	0.006103	0.702026
-31.293811	-1.958805	2.791667	0.006125	0.702072
-31.101044	-1.994587	2.801664	0.006089	0.702069
-30.912218	-1.972359	2.811661	0.006054	0.702181
-30.241753	-1.996574	2.821658	0.005930	0.702373
-30.170606	-2.010130	2.831654	0.005917	0.702371
-30.337640	-1.981835	2.841651	0.005948	0.702367
-29.750699	-1.946581	2.851648	0.005840	0.702649
-29.206643	-2.020287	2.861645	0.005739	0.702695
-29.489106	-1.969014	2.871642	0.005792	0.702696
-29.159809	-1.955958	2.881638	0.005731	0.702841
-28.626725	-1.967730	2.891635	0.005632	0.703008
-28.278065	-2.029915	2.901632	0.005567	0.703007
-28.464986	-1.995871	2.911629	0.005602	0.703008
-27.755612	-1.977392	2.921626	0.005471	0.703300
-27.511440	-1.999152	2.931622	0.005426	0.703343
-27.584321	-1.987842	2.941619	0.005440	0.703339
-27.462733	-1.972413	2.951616	0.005417	0.703413
-26.863010	-1.968223	2.961613	0.005306	0.703637
-26.573186	-2.020574	2.971610	0.005253	0.703635
-26.665276	-2.004408	2.981606	0.005270	0.703633
-26.316863	-1.938869	2.991603	0.005206	0.703890
-25.834671	-1.995992	3.001600	0.005116	0.703948
-26.137170	-1.941306	3.011597	0.005173	0.703948
-25.391845	-2.004105	3.021594	0.005034	0.704089
-24.890779	-2.008726	3.031590	0.004942	0.704259
-25.287561	-1.937542	3.041587	0.005016	0.704259
-24.937836	-1.999602	3.051584	0.004951	0.704259
-24.282585	-1.959442	3.061581	0.004829	0.704575
-24.011850	-1.999042	3.071578	0.004779	0.704591
-24.091707	-1.984360	3.081574	0.004795	0.704592
-24.013547	-1.934934	3.091571	0.004780	0.704718
-23.095010	-2.016498	3.101568	0.004610	0.704883
-23.358685	-1.967649	3.111565	0.004659	0.704886
-23.215334	-1.992644	3.121562	0.004633	0.704887
-22.688172	-1.933342	3.131558	0.004535	0.705195
-22.339836	-1.987154	3.141555	0.004471	0.705211
-22.194613	-2.012054	3.151552	0.004444	0.705212
-22.254244	-1.932065	3.161549	0.004456	0.705351
-21.049216	-2.056578	3.171546	0.004232	0.705532
-21.350863	-2.003835	3.181542	0.004288	0.705529
-21.367421	-2.001836	3.191539	0.004292	0.705526
-20.964776	-1.950494	3.201536	0.004217	0.705773
-20.670498	-1.957319	3.211533	0.004163	0.705864
-20.389096	-2.006533	3.221530	0.004111	0.705865
-20.521948	-1.952483	3.231526	0.004136	0.705926
-19.849629	-1.970559	3.241523	0.004011	0.706130
-19.773482	-1.983065	3.251520	0.003997	0.706131
-19.839062	-1.971241	3.261517	0.004010	0.706130
-19.078302	-1.963479	3.271514	0.003868	0.706418
-18.934955	-1.975169	3.281510	0.003842	0.706445
-18.782019	-2.003113	3.291507	0.003814	0.706443
-18.783301	-1.931377	3.301504	0.003815	0.706586
-17.973826	-1.992552	3.311501	0.003664	0.706752
-17.984051	-1.989817	3.321498	0.003667	0.706753
-18.035589	-1.974699	3.331494	0.003677	0.706764
-17.093125	-1.985209	3.341491	0.003502	0.707080
-16.831673	-2.031484	3.351488	0.003453	0.707080
-17.041610	-1.992489	3.361485	0.003493	0.707082
-16.841045	-1.978118	3.371482	0.003456	0.707182
-15.986017	-2.032027	3.381478	0.003297	0.707379
-16.157226	-2.003285	3.391475	0.003329	0.707375
-16.215461	-1.991564	3.401472	0.003340	0.707377
-15.590466	-1.995169	3.411469	0.003224	0.707592
-15.061742	-2.032587	3.421466	0.003126	0.707705
-15.310384	-1.989149	3.431462	0.003173	0.707703
-15.048760	-2.033037	3.441459	0.003125	0.707708
-14.674078	-1.946130	3.451456	0.003055	0.708015
-14.274511	-2.015850	3.461453	0.002981	0.708017
-14.416518	-1.989120	3.471450	0.003008	0.708020
-14.098432	-1.947742	3.481446	0.002949	0.708215
-13.367401	-2.008565	3.491443	0.002814	0.708354
-13.568454	-1.973066	3.501440	0.002851	0.708352
-13.430931	-1.982740	3.511437	0.002826	0.708381
-12.600504	-1.998679	3.521434	0.002672	0.708645
-12.583950	-2.002510	3.531430	0.002669	0.708643
-12.480685	-2.019767	3.541427	0.002650	0.708644
-12.428851	-1.949968	3.551424	0.002641	0.708802
-11.481358	-2.040912	3.561421	0.002465	0.708957
-11.764401	-1.988576	3.571418	0.002518	0.708960
-11.637091	-2.011602	3.581414	0.002495	0.708959
-11.014223	-1.980940	3.591411	0.002379	0.709242
-10.774593	-2.011877	3.601408	0.002335	0.709264
-10.747180	-2.015458	3.611405	0.002330	0.709266
-10.661608	-1.957067	3.621402	0.002315	0.709413
-9.814742	-2.015504	3.631398	0.002157	0.709597
-9.771294	-2.023974	3.641395	0.002150	0.709595
-10.036227	-1.976665	3.651392	0.002199	0.709594
-8.991783	-2.041440	3.661389	0.002005	0.709836
-9.083131	-1.996337	3.671386	0.002023	0.709893
-8.738684	-2.056651	3.681382	0.001959	0.709895
-9.006759	-2.001590	3.691379	0.002009	0.709909
-8.139495	-2.001723	3.701376	0.001848	0.710216
-7.899115	-2.043920	3.711373	0.001804	0.710217
-7.982587	-2.027934	3.721370	0.001820	0.710219
-7.550160	-2.055817	3.731366	0.001740	0.710316
-6.907554	-2.062225	3.741363	0.001620	0.710531
-6.755128	-2.091565	3.751360	0.001592	0.710526
-6.652704	-2.106672	3.761357	0.001574	0.710532
-6.765882	-2.045010	3.771354	0.001595	0.710614
-5.785975	-2.089359	3.781350	0.001413	0.710873
-5.914668	-2.066684	3.791347	0.001437	0.710872
-5.878414	-2.073404	3.801344	0.001431	0.710871
-5.965792	-2.011073	3.811341	0.001448	0.710963
-5.259094	-2.049239	3.821338	0.001316	0.711138
-5.048073	-2.087298	3.831334	0.001278	0.711136
-5.543760	-1.994605	3.841331	0.001370	0.711144
-4.485464	-2.029151	3.851328	0.001174	0.711451
-4.230474	-2.072694	3.861325	0.001127	0.711454
-4.434566	-2.036703	3.871322	0.001165	0.711452
-3.971554	-2.030085	3.881318	0.001079	0.711629
-3.520708	-2.044521	3.891315	0.000995	0.711760
-3.387980	-2.067844	3.901312	0.000971	0.711760
-3.345534	-2.072296	3.911309	0.000964	0.711765
-2.650483	-2.032161	3.921306	0.000835	0.712091
-2.308038	-2.093754	3.931302	0.000771	0.712090
-2.743831	-2.016637	3.941299	0.000853	0.712088
-2.361341	-2.026573	3.951296	0.000782	0.712203
-1.578548	-2.074360	3.961293	0.000637	0.712385
-1.730916	-2.045863	3.971290	0.000665	0.712387
-1.760666	-2.040705	3.981286	0.000671	0.712386
-1.509511	-1.929096	3.991283	0.000625	0.712697
-1.298749	-1.959727	4.001280	0.000586	0.712710
-1.261960	-1.958613	4.011277	0.000579	0.712724
-1.057850	-1.842433	4.021274	0.000542	0.713027
-1.077627	-1.838934	4.031270	0.000546	0.713026
-1.001825	-1.770224	4.041267	0.000532	0.713189
-0.938003	-1.696098	4.051264	0.000520	0.713359
-0.790007	-1.684694	4.061261	0.000493	0.713433
-0.667861	-1.596405	4.071258	0.000471	0.713651
-0.685495	-1.553863	4.081254	0.000475	0.713729
-0.420381	-1.480067	4.091251	0.000426	0.713968
-0.605887	-1.389548	4.101248	0.000460	0.714082
-0.450623	-1.318506	4.111245	0.000432	0.714277
-0.435752	-1.211170	4.121242	0.000429	0.714495
-0.170568	-1.196101	4.131238	0.000380	0.714618
-0.232137	-1.037925	4.141235	0.000392	0.714910
-0.199300	-0.963349	4.151232	0.000386	0.715068
-0.126547	-0.881251	4.161229	0.000373	0.715256
-0.165510	-0.724646	4.171226	0.000381	0.715552
-0.222062	-0.591538	4.181222	0.000391	0.715796
-0.141087	-0.499844	4.191219	0.000377	0.716005
0.002332	-0.424805	4.201216	0.000350	0.716204
0.079326	-0.308824	4.211213	0.000336	0.716460
-0.029950	-0.137864	4.221210	0.000357	0.716759
0.199504	-0.029903	4.231206	0.000315	0.717053
0.193117	0.105866	4.241203	0.000316	0.717319
0.000000	0.304881	4.251200	0.000352	0.717644
0.175047	0.923407	4.256205	0.000319	0.718927
0.483139	2.117597	4.261210	0.000261	0.721387
0.689380	3.918194	4.266214	0.000222	0.724992
0.760449	6.305279	4.271219	0.000207	0.729673
0.896135	9.181985	4.276224	0.000181	0.735291
1.221834	12.496815	4.281229	0.000118	0.741771
1.715606	16.246150	4.286234	0.000024	0.749074
1.913695	20.453887	4.291238	-0.000016	0.757068
2.281245	25.018714	4.296243	-0.000087	0.765696
2.653164	29.959514	4.301248	-0.000159	0.774917
3.047873	35.233589	4.306253	-0.000236	0.784640
3.374359	40.854230	4.311258	-0.000300	0.794842
3.929059	46.716166	4.316262	-0.000407	0.805410
4.440321	52.892989	4.321267	-0.000506	0.816375
5.112049	59.296718	4.326272	-0.000635	0.827632
5.724954	65.964837	4.331277	-0.000753	0.839167
6.349386	72.839554	4.336282	-0.000874	0.850893
8.689830	79.629758	4.341286	-0.001314	0.862818
9.145683	86.976027	4.346291	-0.001404	0.874943
9.868113	94.428189	4.351296	-0.001543	0.887146
11.207022	101.949632	4.356301	-0.001797	0.899463
11.994755	109.728468	4.361306	-0.001948	0.911863
13.025661	117.570447	4.366310	-0.002145	0.924258
13.878624	125.580292	4.371315	-0.002309	0.936696
14.972584	133.649681	4.376320	-0.002518	0.949122
15.930412	141.835649	4.381325	-0.002701	0.961523
16.824871	150.126772	4.386330	-0.002873	0.973904
17.871319	158.458229	4.391334	-0.003073	0.986224
19.065052	166.856853	4.396339	-0.003301	0.998524
20.056530	175.299629	4.401344	-0.003491	1.010686
21.357540	183.740926	4.406349	-0.003738	1.022775
22.172826	192.329337	4.411354	-0.003895	1.034808
22.680909	200.961014	4.416358	-0.003995	1.046689
23.150012	209.650729	4.421363	-0.004088	1.058505
23.857827	218.302089	4.426368	-0.004225	1.070194
24.909759	226.891535	4.431373	-0.004427	1.081753
25.981463	235.512083	4.436378	-0.004632	1.093234
26.820564	244.167289	4.441382	-0.004793	1.104589
27.612660	252.856019	4.446387	-0.004946	1.115859
28.287445	261.530128	4.451392	-0.005077	1.126973
29.002223	270.211556	4.456397	-0.005216	1.137996
29.862469	278.876530	4.461402	-0.005382	1.148922
30.615519	287.532636	4.466406	-0.005527	1.159712
31.391823	296.154203	4.471411	-0.005677	1.170366
32.247543	304.749051	4.476416	-0.005842	1.180907
33.049034	313.353572	4.481421	-0.005997	1.191354
33.700949	321.973103	4.486426	-0.006124	1.201698
34.029945	330.619475	4.491430	-0.006190	1.211921
34.947626	339.166744	4.496435	-0.006366	1.222059
35.728976	347.742670	4.501440	-0.006517	1.232120
36.428311	356.287145	4.506445	-0.006653	1.242046
37.038335	364.843000	4.511450	-0.006772	1.251890
37.368536	373.413337	4.516454	-0.006839	1.261620
38.108852	381.917692	4.521459	-0.006982	1.271278
38.956271	390.375548	4.526464	-0.007145	1.280832
39.599764	398.869615	4.531469	-0.007270	1.290317
40.636517	407.298751	4.536474	-0.007469	1.299734
41.342743	415.791466	4.541478	-0.007605	1.309091
41.845790	424.380195	4.546483	-0.007705	1.318448
42.490420	432.786840	4.551488	-0.007830	1.327570
43.769247	441.106314	4.556493	-0.008073	1.336649
44.554939	449.498051	4.561498	-0.008225	1.345656
45.223099	457.913117	4.566502	-0.008354	1.354606
45.496725	466.361706	4.571507	-0.008411	1.363464
45.916441	474.790370	4.576512	-0.008494	1.372269
46.611036	483.140595	4.581517	-0.008629	1.380985
47.728658	491.448889	4.586522	-0.008842	1.389674
48.149991	499.855424	4.591526	-0.008926	1.398291
48.818638	508.191124	4.596531	-0.009056	1.406825
49.769119	516.497099	4.601536	-0.009238	1.415325
50.305467	524.844475	4.606541	-0.009343	1.423746
50.846267	533.210628	4.611546	-0.009449	1.432137
51.341740	541.531503	4.616550	-0.009546	1.440427
52.250329	549.815350	4.621555	-0.009721	1.448699
52.734175	558.162673	4.626560	-0.009816	1.456918
53.319359	566.461338	4.631565	-0.009930	1.465060
54.161346	574.787302	4.636570	-0.010092	1.473223
54.607725	583.097035	4.641574	-0.010181	1.481263
55.146580	591.390364	4.646579	-0.010286	1.489259
55.678053	599.689670	4.651584	-0.010390	1.497216
56.126071	607.958963	4.656589	-0.010479	1.505090
56.615120	616.258681	4.661594	-0.010575	1.512957
57.393244	624.455695	4.666598	-0.010725	1.520732
57.679402	632.763247	4.671603	-0.010784	1.528495
58.210106	641.024993	4.676608	-0.010888	1.536214
58.665982	649.278550	4.681613	-0.010978	1.543874
59.142121	657.554203	4.686618	-0.011072	1.551520
59.758413	665.766868	4.691622	-0.011192	1.559092
60.494763	673.965983	4.696627	-0.011334	1.566632
61.227376	682.186887	4.701632	-0.011475	1.574155
62.116011	690.354744	4.706637	-0.011646	1.581617
62.709101	698.603036	4.711642	-0.011762	1.589072
63.150964	706.850046	4.716646	-0.011849	1.596470
63.491600	715.098235	4.721651	-0.011918	1.603820
63.940339	723.336475	4.726656	-0.012006	1.611144
64.253395	731.582784	4.731661	-0.012070	1.618421
64.782505	739.787797	4.736666	-0.012174	1.625661
65.179363	748.046309	4.741670	-0.012253	1.632896
65.847315	756.221315	4.746675	-0.012382	1.640064
66.334624	764.405400	4.751680	-0.012478	1.647184
66.918548	772.597333	4.756685	-0.012592	1.654293
67.322831	780.813295	4.761690	-0.012672	1.661367
67.577488	789.021782	4.766694	-0.012725	1.668385
68.164212	797.205460	4.771699	-0.012839	1.675397
68.511028	805.395540	4.776704	-0.012909	1.682353
68.748294	813.594442	4.781709	-0.012958	1.689273
69.476361	821.746143	4.786714	-0.013099	1.696190
69.875582	829.916068	4.791718	-0.013179	1.703050
70.304807	838.110142	4.796723	-0.013264	1.709907
70.693592	846.313309	4.801728	-0.013341	1.716739
71.338160	854.415913	4.806733	-0.013466	1.723494
71.833057	862.590714	4.811738	-0.013564	1.730262
72.075189	870.790421	4.816742	-0.013614	1.736991
72.792813	878.915056	4.821747	-0.013753	1.743694
73.249554	887.078955	4.826752	-0.013843	1.750370
73.608449	895.264820	4.831757	-0.013915	1.757025
74.213883	903.401073	4.836762	-0.014032	1.763647
74.567813	911.574755	4.841766	-0.014104	1.770242
74.654353	919.798203	4.846771	-0.014125	1.776819
74.842138	927.976348	4.851776	-0.014165	1.783348
75.580746	936.082395	4.856781	-0.014308	1.789864
76.173248	944.264552	4.861786	-0.014423	1.796398
76.349932	952.408541	4.866790	-0.014461	1.802828
76.786439	960.543217	4.871795	-0.014547	1.809259
77.363409	968.670175	4.876800	-0.014660	1.815678
77.603755	976.819948	4.881805	-0.014710	1.822052
78.179781	984.954458	4.886810	-0.014822	1.828431
78.592521	993.097967	4.891814	-0.014904	1.834776
79.073255	1001.218226	4.896819	-0.014999	1.841089
79.569813	1009.353201	4.901824	-0.015096	1.847393
80.092443	1017.494472	4.906829	-0.015199	1.853683
80.583672	1025.638367	4.911834	-0.015295	1.859951
80.483671	1033.821384	4.916838	-0.015282	1.866158
81.074213	1041.972187	4.921843	-0.015397	1.872400
81.545774	1050.097027	4.926848	-0.015490	1.878588
81.995730	1058.172814	4.931853	-0.015579	1.884716
82.436218	1066.303854	4.936858	-0.015666	1.890865
82.678584	1074.449205	4.941862	-0.015716	1.896981
83.062163	1082.570921	4.946867	-0.015793	1.903077
83.399982	1090.705134	4.951872	-0.015861	1.909157
83.917419	1098.808649	4.956877	-0.015962	1.915214
84.331090	1106.929405	4.961882	-0.016044	1.921254
84.598780	1115.055205	4.966886	-0.016099	1.927262
85.105881	1123.177785	4.971891	-0.016199	1.933276
85.595223	1131.291800	4.976896	-0.016295	1.939262
85.922947	1139.407796	4.981901	-0.016361	1.945214
86.321047	1147.570444	4.986906	-0.016440	1.951189
86.691308	1155.698558	4.991910	-0.016514	1.957117
87.195359	1163.769937	4.996915	-0.016613	1.963001
87.326406	1171.912199	5.001920	-0.016643	1.968878
87.565407	1180.036455	5.006925	-0.016692	1.974737
88.182572	1188.101584	5.011930	-0.016812	1.980575
88.586475	1196.183822	5.016934	-0.016893	1.986387
88.908625	1204.327948	5.021939	-0.016958	1.992216
89.473657	1212.409465	5.026944	-0.017068	1.998010
89.860215	1220.495661	5.031949	-0.017145	2.003771
90.442727	1228.596162	5.036954	-0.017259	2.009546
91.026653	1236.685586	5.041958	-0.017372	2.015297
91.417492	1244.793041	5.046963	-0.017450	2.021023
91.682007	1252.937106	5.051968	-0.017505	2.026746
92.054093	1261.056298	5.056973	-0.017579	2.032447
92.532143	1269.167056	5.061978	-0.017673	2.038137
92.804245	1277.263303	5.066982	-0.017729	2.043779
93.200448	1285.357846	5.071987	-0.017808	2.049417
93.787908	1293.449931	5.076992	-0.017922	2.055058
93.790133	1301.578578	5.081997	-0.017928	2.060649
94.285313	1309.661824	5.087002	-0.018025	2.066243
94.323866	1317.817589	5.092006	-0.018037	2.071826
94.756948	1325.890005	5.097011	-0.018123	2.077376
95.008518	1333.984372	5.102016	-0.018175	2.082909
95.283860	1342.060625	5.107021	-0.018231	2.088416
96.113008	1350.122367	5.112026	-0.018391	2.093954
96.369764	1358.226119	5.117030	-0.018444	2.099449
96.750503	1366.313401	5.122035	-0.018520	2.104931
97.361558	1374.412051	5.127040	-0.018638	2.110428
97.476661	1382.577316	5.132045	-0.018665	2.115908
97.785494	1390.658468	5.137050	-0.018728	2.121336
98.001034	1398.736002	5.142054	-0.018773	2.126738
98.420370	1406.809887	5.147059	-0.018856	2.132144
98.692634	1414.916287	5.152064	-0.018912	2.137544
99.023372	1422.974038	5.157069	-0.018978	2.142903
99.543694	1431.048532	5.162074	-0.019080	2.148278
99.866789	1439.158798	5.167078	-0.019146	2.153644
100.137729	1447.250322	5.172083	-0.019201	2.158980
100.428079	1455.316339	5.177088	-0.019260	2.164288
100.637856	1463.420085	5.182093	-0.019304	2.169599
101.072710	1471.510168	5.187098	-0.019390	2.174910
101.141675	1479.607158	5.192102	-0.019408	2.180178
101.675561	1487.649897	5.197107	-0.019513	2.185441
101.784453	1495.797279	5.202112	-0.019538	2.190720
101.844385	1503.905686	5.207117	-0.019554	2.195957
102.460247	1511.931181	5.212122	-0.019674	2.201178
103.090899	1519.949039	5.217126	-0.019797	2.206384
103.261061	1528.072395	5.222131	-0.019833	2.211602
103.713773	1536.142806	5.227136	-0.019923	2.216801
104.268086	1544.189795	5.232141	-0.020031	2.221981
104.413077	1552.315112	5.237146	-0.020063	2.227162
104.734174	1560.401061	5.242150	-0.020128	2.232321
105.264644	1568.461865	5.247155	-0.020232	2.237472
105.498444	1576.543241	5.252160	-0.020280	2.242597
105.712105	1584.620552	5.257165	-0.020325	2.247706
106.168925	1592.718823	5.262170	-0.020415	2.252838
106.528409	1600.772712	5.267174	-0.020487	2.257922
106.373257	1608.909761	5.272179	-0.020464	2.263002
106.751579	1616.957971	5.277184	-0.020539	2.268061
107.015936	1625.096391	5.282189	-0.020593	2.273155
107.397575	1633.162142	5.287194	-0.020670	2.278202
107.786084	1641.174072	5.292198	-0.020747	2.283206
108.203228	1649.215815	5.297203	-0.020830	2.288219
108.275125	1657.333672	5.302208	-0.020848	2.293239
108.652357	1665.363993	5.307213	-0.020923	2.298220
109.178807	1673.414895	5.312218	-0.021027	2.303215
109.268570	1681.514502	5.317222	-0.021048	2.308192
109.527101	1689.611108	5.322227	-0.021102	2.313171
110.007212	1697.656683	5.327232	-0.021196	2.318127
110.233106	1705.710183	5.332237	-0.021243	2.323055
110.440941	1713.796001	5.337242	-0.021287	2.327992
110.745419	1721.859976	5.342246	-0.021349	2.332912
111.021250	1729.940705	5.347251	-0.021405	2.337830
111.408921	1737.999164	5.352256	-0.021482	2.342733
111.577019	1746.072166	5.357261	-0.021519	2.347617
112.159848	1754.147493	5.362266	-0.021632	2.352525
112.801465	1762.163211	5.367270	-0.021757	2.357392
113.161048	1770.217063	5.372275	-0.021829	2.362249
113.573052	1778.290080	5.377280	-0.021911	2.367112
113.504372	1786.401754	5.382285	-0.021903	2.371949
113.796538	1794.493520	5.387290	-0.021962	2.376793
113.849505	1802.567084	5.392294	-0.021977	2.381598
114.120938	1810.611395	5.397299	-0.022033	2.386393
114.398965	1818.695204	5.402304	-0.022090	2.391202
114.735294	1826.753849	5.407309	-0.022157	2.395991
115.397179	1834.762896	5.412314	-0.022286	2.400766
115.618033	1842.811783	5.417318	-0.022332	2.405521
115.942594	1850.891948	5.422323	-0.022397	2.410293
116.210934	1858.991020	5.427328	-0.022452	2.415062
116.545012	1867.035882	5.432333	-0.022520	2.419796
116.569200	1875.156225	5.437338	-0.022529	2.424539
116.906176	1883.190816	5.442342	-0.022597	2.429248
117.297370	1891.322439	5.447347	-0.022675	2.434008
117.819938	1899.340962	5.452352	-0.022777	2.438703
117.747940	1907.395585	5.457357	-0.022769	2.443365
118.211273	1915.436787	5.462362	-0.022860	2.448051
118.356068	1923.515213	5.467366	-0.022892	2.452725
118.751480	1931.544031	5.472371	-0.022971	2.457380
119.170946	1939.596058	5.477376	-0.023054	2.462042
119.512297	1947.634084	5.482381	-0.023123	2.466681
119.963082	1955.707011	5.487386	-0.023212	2.471339
120.163609	1963.782982	5.492390	-0.023254	2.475971
120.439206	1971.827762	5.497395	-0.023311	2.480583
120.668462	1979.893716	5.502400	-0.023358	2.485194
120.823431	1987.934152	5.507405	-0.023392	2.489777
120.985579	1996.060160	5.512410	-0.023428	2.494401
121.474755	2004.064466	5.517414	-0.023524	2.498971
121.440442	2012.141931	5.522419	-0.023522	2.503535
121.688323	2020.221832	5.527424	-0.023574	2.508114
122.077882	2028.275960	5.532429	-0.023651	2.512679
122.531016	2036.315704	5.537434	-0.023741	2.517233
122.881467	2044.336435	5.542438	-0.023811	2.521760
123.446137	2052.351051	5.547443	-0.023921	2.526291
123.959394	2060.417443	5.552448	-0.024022	2.530840
124.267491	2068.480663	5.557453	-0.024084	2.535363
124.543805	2076.541230	5.562458	-0.024141	2.539875
124.919407	2084.584286	5.567462	-0.024216	2.544375
125.089737	2092.670739	5.572467	-0.024252	2.548878
125.177392	2100.792528	5.577472	-0.024274	2.553386
125.668510	2108.788368	5.582477	-0.024370	2.557845
126.111282	2116.809679	5.587482	-0.024458	2.562307
126.184494	2124.885151	5.592486	-0.024476	2.566764
126.666417	2132.925702	5.597491	-0.024571	2.571224
127.304024	2140.992465	5.602496	-0.024695	2.575700
127.451443	2149.045309	5.607501	-0.024728	2.580128
127.733414	2157.087768	5.612506	-0.024785	2.584551
128.180007	2165.151266	5.617510	-0.024873	2.588989
128.515347	2173.365062	5.622515	-0.024941	2.593494
128.821611	2181.412861	5.627520	-0.025003	2.597899
128.981574	2189.403713	5.632525	-0.025038	2.602256
129.602230	2197.418280	5.637530	-0.025158	2.606649
129.788161	2205.470854	5.642534	-0.025198	2.611026
130.259039	2213.504842	5.647539	-0.025291	2.615404
130.678567	2221.531476	5.652544	-0.025374	2.619768
130.811535	2229.585217	5.657549	-0.025404	2.624120
131.141537	2237.643726	5.662554	-0.025470	2.628480
131.179082	2245.722272	5.667558	-0.025482	2.632825
131.427122	2253.762047	5.672563	-0.025534	2.637155
131.633115	2261.805200	5.677568	-0.025577	2.641477
131.830154	2269.824492	5.682573	-0.025619	2.645779
132.228000	2277.866855	5.687578	-0.025698	2.650099
132.536645	2285.908305	5.692582	-0.025760	2.654406
132.733272	2293.959087	5.697587	-0.025802	2.658704
133.156732	2302.000035	5.702592	-0.025886	2.663004
133.289191	2310.045527	5.707597	-0.025916	2.667280
133.621708	2318.145158	5.712602	-0.025983	2.671591
133.794387	2326.215449	5.717606	-0.026020	2.675870
134.068378	2334.221375	5.722611	-0.026076	2.680114
134.407193	2342.242979	5.727616	-0.026144	2.684363
134.506166	2350.301152	5.732621	-0.026167	2.688610
134.825831	2358.375227	5.737626	-0.026232	2.692873
135.047039	2366.416380	5.742630	-0.026278	2.697105
135.281413	2374.442467	5.747635	-0.026327	2.701323
135.563309	2382.498837	5.752640	-0.026385	2.705554
135.890920	2390.525404	5.757645	-0.026451	2.709765
136.073661	2398.610168	5.762650	-0.026490	2.713991
136.445817	2406.630981	5.767654	-0.026564	2.718189
136.709999	2414.647238	5.772659	-0.026618	2.722371
136.977727	2422.717107	5.777664	-0.026673	2.726575
137.050408	2430.772133	5.782669	-0.026692	2.730753
137.572627	2438.819383	5.787674	-0.026794	2.734947
137.818023	2446.862507	5.792678	-0.026845	2.739116
137.997091	2454.896196	5.797683	-0.026883	2.743270
138.538203	2462.923664	5.802688	-0.026989	2.747437
138.787381	2470.993817	5.807693	-0.027040	2.751601
138.934963	2479.142478	5.812698	-0.027073	2.755793
139.065816	2487.134320	5.817702	-0.027102	2.759897
139.404584	2495.132048	5.822707	-0.027170	2.764010
139.792896	2503.184994	5.827712	-0.027248	2.768149
139.883499	2511.228104	5.832717	-0.027270	2.772258
140.521844	2519.248669	5.837722	-0.027394	2.776383
140.496094	2527.312286	5.842726	-0.027394	2.780484
140.736248	2535.326097	5.847731	-0.027444	2.784569
141.057359	2543.391070	5.852736	-0.027509	2.788679
141.563368	2551.417687	5.857741	-0.027608	2.792774
141.974871	2559.472882	5.862746	-0.027689	2.796872
142.389622	2567.487167	5.867750	-0.027772	2.800943
142.761619	2575.504656	5.872755	-0.027846	2.805008
142.951444	2583.586625	5.877760	-0.027886	2.809088
143.136539	2591.649933	5.882765	-0.027926	2.813153
143.560689	2599.677027	5.887770	-0.028010	2.817207
143.735745	2607.727036	5.892774	-0.028048	2.821253
144.069831	2615.744917	5.897779	-0.028115	2.825286
144.386453	2623.812690	5.902784	-0.028179	2.829337
144.771285	2631.871913	5.907789	-0.028256	2.833382
144.874405	2639.942983	5.912794	-0.028280	2.837411
145.082187	2647.957831	5.917798	-0.028324	2.841412
145.440794	2655.953784	5.922803	-0.028395	2.845407
145.751425	2663.999972	5.927808	-0.028458	2.849418
145.763586	2672.066843	5.932813	-0.028466	2.853417
146.104394	2680.118046	5.937818	-0.028534	2.857421
146.262981	2688.150070	5.942822	-0.028569	2.861400
146.559758	2696.165163	5.947827	-0.028629	2.865372
146.728969	2704.234396	5.952832	-0.028666	2.869359
146.900775	2712.277210	5.957837	-0.028703	2.873327
147.112385	2720.332509	5.962842	-0.028747	2.877298
147.448455	2728.341236	5.967846	-0.028815	2.881247
147.661323	2736.366594	5.972851	-0.028859	2.885192
148.114363	2744.403130	5.977856	-0.028949	2.889151
148.211113	2752.479030	5.982861	-0.028972	2.893103
148.609101	2760.529418	5.987866	-0.029051	2.897055
148.691393	2768.567016	5.992870	-0.029071	2.900977
148.924099	2776.579023	5.997875	-0.029120	2.904890
149.340407	2784.635043	6.002880	-0.029202	2.908829
149.474713	2792.748077	6.007885	-0.029232	2.912774
149.831477	2800.787806	6.012890	-0.029304	2.916691
150.025973	2808.788601	6.017894	-0.029345	2.920575
150.411979	2816.752039	6.022899	-0.029422	2.924446
150.560524	2824.816261	6.027904	-0.029455	2.928348
150.849816	2832.840329	6.032909	-0.029514	2.932233
151.203809	2840.893448	6.037914	-0.029585	2.936130
151.373359	2848.914520	6.042918	-0.029621	2.939996
151.576555	2856.933488	6.047923	-0.029664	2.943859
151.864731	2864.999481	6.052928	-0.029723	2.947743
152.146835	2873.033889	6.057933	-0.029780	2.951606
152.386507	2881.099235	6.062938	-0.029830	2.955477
152.580641	2889.117430	6.067942	-0.029871	2.959318
152.840824	2897.120059	6.072947	-0.029925	2.963150
153.234944	2905.167969	6.077952	-0.030003	2.967006
153.261579	2913.238397	6.082957	-0.030013	2.970848
153.470245	2921.307699	6.087962	-0.030057	2.974694
154.001186	2929.291928	6.092966	-0.030161	2.978511
154.045295	2937.336622	6.097971	-0.030174	2.982327
154.169446	2945.405564	6.102976	-0.030202	2.986153
154.529415	2953.420234	6.107981	-0.030274	2.989961
154.918704	2961.501082	6.112986	-0.030352	2.993797
155.174947	2969.513859	6.117990	-0.030405	2.997589
155.291473	2977.534444	6.122995	-0.030431	3.001373
155.582549	2985.546808	6.128000	-0.030491	3.005157
155.708899	2993.560176	6.133005	-0.030519	3.008928
156.178062	3001.604899	6.138010	-0.030612	3.012726
156.561096	3009.657729	6.143014	-0.030688	3.016519
156.748437	3017.677985	6.148019	-0.030728	3.020282
157.052146	3025.714900	6.153024	-0.030790	3.024055
157.261867	3033.748399	6.158029	-0.030834	3.027816
157.562034	3041.809384	6.163034	-0.030895	3.031589
157.593899	3049.878940	6.168038	-0.030906	3.035349
157.946899	3057.860077	6.173043	-0.030976	3.039079
158.220056	3065.913265	6.178048	-0.031032	3.042833
158.427659	3073.934174	6.183053	-0.031076	3.046565
158.707890	3081.972372	6.188058	-0.031133	3.050303
158.771145	3090.063163	6.193062	-0.031150	3.054051
159.140631	3098.053411	6.198067	-0.031224	3.057763
159.531467	3106.092645	6.203072	-0.031302	3.061493
159.943393	3114.079447	6.208077	-0.031383	3.065196
160.356167	3122.130973	6.213082	-0.031465	3.068924
160.339898	3130.247795	6.218086	-0.031467	3.072657
160.692467	3138.277126	6.223091	-0.031538	3.076363
161.156824	3146.268897	6.228096	-0.031630	3.080052
161.295622	3154.285094	6.233101	-0.031660	3.083733
161.416731	3162.332524	6.238106	-0.031688	3.087423
161.533193	3170.375089	6.243110	-0.031715	3.091106
161.904814	3178.380394	6.248115	-0.031789	3.094779
162.049041	3186.431975	6.253120	-0.031821	3.098459
162.196043	3194.465505	6.258125	-0.031853	3.102126
162.571036	3202.487837	6.263130	-0.031928	3.105794
162.820511	3210.514534	6.268134	-0.031980	3.109454
162.912993	3218.567180	6.273139	-0.032002	3.113114
163.387612	3226.606445	6.278144	-0.032095	3.116781
163.469197	3234.606223	6.283149	-0.032116	3.120409
163.733654	3242.633806	6.288154	-0.032170	3.124052
163.852420	3250.695699	6.293158	-0.032197	3.127701
164.085933	3258.709361	6.298163	-0.032246	3.131328
164.569906	3266.766631	6.303168	-0.032341	3.134982
164.830830	3274.752148	6.308173	-0.032394	3.138590
165.370036	3282.781462	6.313178	-0.032500	3.142225
165.423041	3290.855509	6.318182	-0.032515	3.145854
165.604056	3298.875571	6.323187	-0.032553	3.149461
166.044508	3306.945795	6.328192	-0.032640	3.153098
166.038607	3314.989527	6.333197	-0.032644	3.156699
166.309419	3322.986891	6.338202	-0.032700	3.160287
166.576528	3330.982656	6.343206	-0.032755	3.163870
166.694066	3339.017518	6.348211	-0.032782	3.167460
167.089286	3347.069059	6.353216	-0.032860	3.171065
167.340804	3355.122080	6.358221	-0.032912	3.174661
167.671812	3363.140177	6.363226	-0.032979	3.178240
167.603747	3371.208649	6.368230	-0.032971	3.181821
167.709112	3379.192098	6.373235	-0.032996	3.185367
168.178518	3387.234951	6.378240	-0.033088	3.188951
168.320988	3395.279507	6.383245	-0.033120	3.192518
168.579351	3403.345405	6.388250	-0.033173	3.196095
168.993339	3411.319382	6.393254	-0.033255	3.199634
169.318130	3419.302369	6.398259	-0.033321	3.203170
169.647450	3427.364800	6.403264	-0.033387	3.206736
169.886435	3435.383177	6.408269	-0.033436	3.210276
170.176943	3443.460371	6.413274	-0.033496	3.213839
170.562602	3451.489358	6.418278	-0.033573	3.217381
170.617979	3459.510717	6.423283	-0.033588	3.220903
171.173408	3467.508258	6.428288	-0.033696	3.224430
171.238994	3475.554248	6.433293	-0.033714	3.227955
171.290905	3483.663925	6.438298	-0.033728	3.231503
171.832518	3491.690436	6.443302	-0.033834	3.235031
172.112671	3499.690868	6.448307	-0.033891	3.238533
172.020818	3507.748237	6.453312	-0.033879	3.242041
172.243100	3515.684759	6.458317	-0.033926	3.245505
172.637481	3523.740389	6.463322	-0.034004	3.249024
172.817326	3531.803161	6.468326	-0.034043	3.252534
172.972960	3539.814340	6.473331	-0.034077	3.256017
173.207345	3547.837036	6.478336	-0.034125	3.259503
173.495323	3555.854877	6.483341	-0.034184	3.262987
173.603378	3563.907992	6.488346	-0.034209	3.266474
173.905114	3571.939814	6.493350	-0.034271	3.269957
174.083030	3579.977148	6.498355	-0.034309	3.273433
174.300520	3588.032565	6.503360	-0.034354	3.276914
174.671205	3595.979791	6.508365	-0.034428	3.280352
174.881858	3604.005188	6.513370	-0.034472	3.283813
175.047205	3612.074503	6.518374	-0.034508	3.287287
175.177360	3620.108319	6.523379	-0.034538	3.290741
175.531548	3628.169115	6.528384	-0.034609	3.294212
175.809040	3636.174017	6.533389	-0.034665	3.297652
176.013657	3644.209995	6.538394	-0.034708	3.301099
176.237389	3652.203819	6.543398	-0.034755	3.304525
176.571877	3660.234220	6.548403	-0.034822	3.307968
176.884361	3668.301467	6.553408	-0.034886	3.311421
176.879996	3676.355556	6.558413	-0.034890	3.314853
177.308351	3684.341552	6.563418	-0.034975	3.318270
177.566124	3692.373820	6.568422	-0.035028	3.321695
177.641254	3700.357816	6.573427	-0.035047	3.325090
177.914995	3708.423814	6.578432	-0.035103	3.328524
178.227162	3716.450704	6.583437	-0.035166	3.331939
178.309367	3724.501687	6.588442	-0.035186	3.335352
178.512434	3732.523832	6.593446	-0.035229	3.338753
178.896806	3740.527379	6.598451	-0.035306	3.342150
179.198678	3748.546432	6.603456	-0.035367	3.345547
179.227928	3756.584844	6.608461	-0.035378	3.348939
179.498764	3764.638687	6.613466	-0.035433	3.352343
179.602880	3772.698180	6.618470	-0.035457	3.355739
179.732590	3780.694611	6.623475	-0.035487	3.359107
180.018431	3788.728094	6.628480	-0.035545	3.362492
180.318269	3796.714283	6.633485	-0.035606	3.365854
180.309376	3804.767061	6.638490	-0.035609	3.369230
180.680516	3812.820082	6.643494	-0.035683	3.372616
180.843310	3820.825221	6.648499	-0.035719	3.375971
181.055988	3828.859575	6.653504	-0.035763	3.379337
181.201957	3836.874042	6.658509	-0.035795	3.382689
181.581527	3844.898485	6.663514	-0.035871	3.386050
181.765562	3852.909366	6.668518	-0.035911	3.389395
181.779168	3861.012380	6.673523	-0.035918	3.392769
182.198902	3869.081092	6.678528	-0.036001	3.396139
182.330208	3877.044628	6.683533	-0.036031	3.399453
182.698282	3885.041353	6.688538	-0.036104	3.402785
182.760940	3893.063290	6.693542	-0.036121	3.406113
183.178875	3901.021316	6.698547	-0.036204	3.409425
183.461325	3909.110231	6.703552	-0.036262	3.412782
183.442192	3917.169531	6.708557	-0.036263	3.416113
183.703169	3925.158343	6.713562	-0.036317	3.419422
183.866332	3933.207746	6.718566	-0.036352	3.422749
183.915478	3941.209283	6.723571	-0.036366	3.426050
184.348607	3949.242418	6.728576	-0.036452	3.429373
184.537931	3957.291367	6.733581	-0.036492	3.432691
184.787871	3965.315894	6.738586	-0.036544	3.435997
184.692982	3973.368765	6.743590	-0.036531	3.439301
184.896451	3981.347225	6.748595	-0.036574	3.442581
185.311920	3989.377172	6.753600	-0.036657	3.445886
185.430767	3997.408511	6.758605	-0.036684	3.449179
185.572983	4005.443409	6.763610	-0.036715	3.452470
186.001858	4013.486664	6.768614	-0.036800	3.455771
186.050318	4021.489570	6.773619	-0.036814	3.459040
186.279517	4029.560640	6.778624	-0.036862	3.462340
186.401618	4037.541541	6.783629	-0.036890	3.465596
186.757238	4045.575071	6.788634	-0.036961	3.468878
187.170041	4053.625657	6.793638	-0.037043	3.472166
187.069653	4061.662525	6.798643	-0.037029	3.475429
187.459256	4069.638889	6.803648	-0.037107	3.478679
187.536465	4077.657575	6.808653	-0.037126	3.481934
187.879962	4085.666689	6.813658	-0.037195	3.485190
188.038708	4093.728063	6.818662	-0.037230	3.488459
188.371029	4101.752585	6.823667	-0.037297	3.491715
188.562507	4109.807362	6.828672	-0.037337	3.494975
188.937735	4117.770317	6.833677	-0.037412	3.498202
189.054917	4125.846838	6.838682	-0.037439	3.501462
189.170087	4133.831880	6.843686	-0.037466	3.504683
189.454462	4141.850029	6.848691	-0.037524	3.507920
189.771476	4149.925235	6.853696	-0.037588	3.511177
189.828088	4157.937971	6.858701	-0.037603	3.514399
190.056659	4165.956555	6.863706	-0.037651	3.517625
190.376863	4173.984937	6.868710	-0.037715	3.520854
190.588092	4181.973048	6.873715	-0.037760	3.524062
190.752147	4190.029871	6.878720	-0.037795	3.527292
190.938568	4198.054976	6.883725	-0.037835	3.530507
191.043550	4206.113987	6.888730	-0.037860	3.533731
191.164027	4214.151075	6.893734	-0.037887	3.536943
191.398125	4222.136059	6.898739	-0.037936	3.540135
191.948203	4230.161805	6.903744	-0.038043	3.543350
191.865797	4238.207262	6.908749	-0.038033	3.546550
192.030547	4246.237529	6.913754	-0.038069	3.549750
192.211862	4254.351693	6.918758	-0.038108	3.552980
192.430825	4262.383209	6.923763	-0.038153	3.556175
192.576156	4270.355087	6.928768	-0.038185	3.559342
192.546899	4278.350221	6.933773	-0.038185	3.562509
192.852955	4286.334002	6.938778	-0.038247	3.565680
193.112845	4294.352909	6.943782	-0.038300	3.568860
193.414897	4302.357820	6.948787	-0.038362	3.572033
193.626210	4310.408280	6.953792	-0.038406	3.575218
193.951217	4318.407840	6.958797	-0.038472	3.578384
194.010787	4326.477567	6.963802	-0.038488	3.581567
194.124260	4334.487145	6.968806	-0.038514	3.584725
194.433915	4342.494381	6.973811	-0.038577	3.587884
194.522166	4350.547078	6.978816	-0.038598	3.591053
194.616534	4358.569917	6.983821	-0.038621	3.594207
194.688054	4366.593538	6.988826	-0.038639	3.597358
194.972435	4374.587456	6.993830	-0.038697	3.600501
194.962995	4382.568060	6.998835	-0.038700	3.603627
195.475044	4390.635681	7.003840	-0.038801	3.606799
195.605399	4398.623599	7.008845	-0.038830	3.609927
195.648039	4406.706266	7.013850	-0.038843	3.613087
195.765331	4414.769950	7.018854	-0.038870	3.616238
195.973112	4422.725444	7.023859	-0.038914	3.619347
196.158348	4430.767200	7.028864	-0.038953	3.622486
196.158732	4438.770442	7.033869	-0.038958	3.625602
196.599133	4446.784301	7.038874	-0.039045	3.628732
196.923850	4454.874425	7.043878	-0.039111	3.631886
197.035466	4462.886842	7.048883	-0.039137	3.635000
197.349939	4470.932355	7.053888	-0.039200	3.638131
197.567889	4478.931206	7.058893	-0.039246	3.641238
197.601204	4486.927159	7.063898	-0.039257	3.644336
197.897896	4494.966688	7.068902	-0.039317	3.647456
198.137415	4502.978393	7.073907	-0.039367	3.650560
198.493667	4511.022188	7.078912	-0.039438	3.653678
198.622771	4519.079619	7.083917	-0.039468	3.656791
198.705671	4527.051574	7.088922	-0.039488	3.659868
198.959126	4535.090030	7.093926	-0.039540	3.662973
199.125232	4543.095910	7.098931	-0.039576	3.666060
199.226612	4551.132469	7.103936	-0.039600	3.669155
199.574317	4559.151984	7.108941	-0.039670	3.672246
199.619266	4567.199537	7.113946	-0.039683	3.675338
199.895029	4575.204276	7.118950	-0.039740	3.678417
200.032605	4583.225064	7.123955	-0.039770	3.681496
200.328504	4591.195640	7.128960	-0.039830	3.684557
200.216378	4599.270199	7.133965	-0.039815	3.687645
200.688829	4607.277733	7.138970	-0.039908	3.690720
200.916694	4615.355682	7.143974	-0.039955	3.693812
201.010448	4623.340527	7.148979	-0.039978	3.696864
201.256892	4631.357218	7.153984	-0.040028	3.699928
201.589427	4639.380783	7.158989	-0.040095	3.702995
201.668532	4647.400596	7.163994	-0.040115	3.706051
201.760807	4655.418829	7.168998	-0.040137	3.709105
202.105435	4663.441346	7.174003	-0.040207	3.712164
202.325929	4671.585524	7.179008	-0.040253	3.715263
202.480271	4679.546688	7.184013	-0.040287	3.718289
202.615085	4687.522251	7.189018	-0.040317	3.721318
202.947214	4695.496703	7.194022	-0.040383	3.724348
202.971019	4703.545298	7.199027	-0.040393	3.727396
203.133535	4711.566093	7.204032	-0.040428	3.730435
203.252120	4719.616117	7.209037	-0.040455	3.733481
203.561877	4727.639201	7.214042	-0.040518	3.736519
203.645762	4735.621947	7.219046	-0.040539	3.739534
203.772510	4743.637473	7.224051	-0.040567	3.742560
204.109123	4751.689515	7.229056	-0.040635	3.745602
204.336305	4759.719415	7.234061	-0.040682	3.748630
204.579017	4767.743327	7.239066	-0.040733	3.751655
204.699488	4775.797193	7.244070	-0.040760	3.754685
204.658372	4783.786120	7.249075	-0.040758	3.757685
204.863070	4791.821200	7.254080	-0.040801	3.760705
204.997818	4799.815493	7.259085	-0.040831	3.763706
205.208457	4807.867434	7.264090	-0.040875	3.766727
205.253877	4815.866782	7.269094	-0.040889	3.769723
205.528318	4823.908681	7.274099	-0.040945	3.772738
205.952814	4831.968094	7.279104	-0.041029	3.775760
206.022054	4839.939393	7.284109	-0.041047	3.778739
206.256198	4847.982403	7.289114	-0.041095	3.781746
206.496511	4855.977112	7.294118	-0.041145	3.784732
206.550616	4864.013701	7.299123	-0.041160	3.787728
206.750540	4872.058050	7.304128	-0.041202	3.790727
207.007528	4880.108829	7.309133	-0.041255	3.793727
207.169521	4888.122157	7.314138	-0.041291	3.796710
207.166771	4896.085164	7.319142	-0.041295	3.799667
207.191689	4904.107453	7.324147	-0.041305	3.802645
207.376618	4912.143500	7.329152	-0.041344	3.805629
207.552086	4920.139294	7.334157	-0.041382	3.808595
207.773498	4928.152222	7.339162	-0.041428	3.811567
208.494015	4936.187248	7.344166	-0.041567	3.814555
208.556882	4944.201925	7.349171	-0.041584	3.817519
208.744932	4952.218177	7.354176	-0.041624	3.820484
208.883440	4960.230900	7.359181	-0.041655	3.823444
208.914705	4968.284842	7.364186	-0.041666	3.826415
209.390288	4976.291710	7.369190	-0.041759	3.829376
209.331145	4984.341370	7.374195	-0.041753	3.832339
209.696928	4992.371432	7.379200	-0.041827	3.835301
209.737258	5000.350665	7.384205	-0.041839	3.838235
209.904794	5008.367116	7.389210	-0.041875	3.841183
210.278194	5016.384200	7.394214	-0.041950	3.844134
210.426965	5024.409966	7.399219	-0.041983	3.847081
210.390220	5032.422478	7.404224	-0.041981	3.850017
210.550063	5040.500100	7.409229	-0.042016	3.852978
210.762480	5048.504291	7.414234	-0.042060	3.855912
211.210570	5056.506795	7.419238	-0.042149	3.858847
211.145835	5064.552340	7.424243	-0.042142	3.861786
211.535105	5072.544897	7.429248	-0.042219	3.864712
211.483196	5080.601162	7.434253	-0.042215	3.867650
211.675063	5088.619432	7.439258	-0.042255	3.870577
211.803924	5096.854761	7.444262	-0.042285	3.873579
212.067062	5104.855046	7.449267	-0.042339	3.876496
212.319185	5112.776200	7.454272	-0.042390	3.879382
212.466552	5120.757966	7.459277	-0.042423	3.882286
212.585031	5128.692283	7.464282	-0.042450	3.885170
212.673018	5136.794251	7.469286	-0.042471	3.888112
212.733318	5144.760035	7.474291	-0.042488	3.891001
213.048070	5152.819170	7.479296	-0.042551	3.893928
213.127404	5160.829625	7.484301	-0.042571	3.896829
213.219167	5168.803142	7.489306	-0.042593	3.899716
213.431029	5176.857539	7.494310	-0.042638	3.902632
213.705250	5184.849971	7.499315	-0.042694	3.905525
213.971050	5192.886957	7.504320	-0.042748	3.908431
214.186200	5200.918810	7.509325	-0.042793	3.911332
214.456825	5208.950403	7.514330	-0.042849	3.914232
214.667377	5216.948669	7.519334	-0.042893	3.917117
214.655483	5224.915701	7.524339	-0.042896	3.919984
215.005980	5232.994298	7.529344	-0.042966	3.922896
215.097489	5240.969655	7.534349	-0.042988	3.925764
215.146172	5248.972184	7.539354	-0.043002	3.928639
215.672562	5257.062744	7.544358	-0.043105	3.931551
215.803171	5265.049600	7.549363	-0.043135	3.934418
216.035825	5273.099131	7.554368	-0.043183	3.937306
216.160636	5281.057990	7.559373	-0.043211	3.940158
216.079388	5289.098349	7.564378	-0.043201	3.943034
216.405787	5297.141904	7.569382	-0.043267	3.945915
216.612289	5305.122200	7.574387	-0.043311	3.948770
216.900262	5313.178735	7.579392	-0.043369	3.951651
217.135939	5321.240328	7.584397	-0.043418	3.954531
217.208835	5329.215061	7.589402	-0.043437	3.957375
217.372812	5337.204313	7.594406	-0.043472	3.960224
217.629956	5345.214207	7.599411	-0.043525	3.963080
218.096221	5353.237520	7.604416	-0.043617	3.965942
218.208381	5361.285513	7.609421	-0.043643	3.968804
218.502520	5369.283229	7.614426	-0.043703	3.971650
218.806065	5377.299565	7.619430	-0.043764	3.974501
218.905633	5385.337583	7.624435	-0.043788	3.977353
219.188312	5393.319942	7.629440	-0.043846	3.980187
219.392909	5401.369090	7.634445	-0.043889	3.983041
219.208730	5409.397222	7.639450	-0.043860	3.985879
219.632576	5417.414260	7.644454	-0.043943	3.988722
219.842035	5425.440044	7.649459	-0.043988	3.991561
220.039548	5433.511099	7.654464	-0.044029	3.994415
220.074173	5441.525569	7.659469	-0.044041	3.997244
220.101256	5449.546967	7.664474	-0.044051	4.000073
220.388983	5457.572852	7.669478	-0.044110	4.002906
220.267440	5465.523742	7.674483	-0.044092	4.005704
220.623055	5473.550944	7.679488	-0.044163	4.008534
220.821458	5481.622116	7.684493	-0.044205	4.011375
220.937547	5489.640564	7.689498	-0.044232	4.014195
221.181311	5497.685708	7.694502	-0.044282	4.017024
221.654520	5505.656162	7.699507	-0.044375	4.019828
221.748503	5513.695419	7.704512	-0.044398	4.022648
221.892075	5521.709666	7.709517	-0.044430	4.025459
222.115464	5529.715391	7.714522	-0.044476	4.028265
222.391404	5537.781637	7.719526	-0.044533	4.031092
222.259954	5545.868629	7.724531	-0.044513	4.033918
222.558565	5553.864944	7.729536	-0.044574	4.036716
222.768756	5561.827803	7.734541	-0.044618	4.039500
222.984249	5569.810342	7.739546	-0.044663	4.042289
223.000179	5577.829369	7.744550	-0.044671	4.045085
223.179995	5585.829094	7.749555	-0.044710	4.047875
223.236984	5593.853948	7.754560	-0.044725	4.050670
223.741877	5601.911363	7.759565	-0.044824	4.053481
223.947624	5609.934985	7.764570	-0.044868	4.056274
224.327282	5617.919255	7.769574	-0.044943	4.059054
224.592615	5625.939975	7.774579	-0.044998	4.061843
224.739313	5633.940607	7.779584	-0.045030	4.064621
224.868473	5641.974518	7.784589	-0.045059	4.067409
225.041863	5649.968938	7.789594	-0.045097	4.070181
224.935824	5658.052378	7.794598	-0.045082	4.072979
225.415606	5666.060823	7.799603	-0.045176	4.075757
225.607259	5674.069359	7.804608	-0.045217	4.078529
225.866794	5682.092464	7.809613	-0.045270	4.081305
226.195669	5690.042419	7.814618	-0.045337	4.084055
226.521843	5698.112917	7.819622	-0.045402	4.086845
226.705882	5706.111356	7.824627	-0.045442	4.089605
226.843903	5714.173275	7.829632	-0.045473	4.092385
227.003460	5722.182768	7.834637	-0.045507	4.095146
227.035546	5730.181815	7.839642	-0.045518	4.097899
227.210253	5738.218893	7.844646	-0.045556	4.100666
227.577479	5746.185017	7.849651	-0.045629	4.103408
227.812097	5754.223534	7.854656	-0.045678	4.106172
227.854628	5762.254860	7.859661	-0.045691	4.108929
227.983174	5770.291992	7.864666	-0.045720	4.111688
228.235107	5778.353626	7.869670	-0.045772	4.114454
228.305786	5786.359203	7.874675	-0.045790	4.117197
228.535270	5794.337778	7.879680	-0.045838	4.119931
228.757255	5802.370421	7.884685	-0.045884	4.122681
228.867845	5810.313052	7.889690	-0.045910	4.125398
228.996853	5818.427596	7.894694	-0.045939	4.128171
229.018235	5826.423508	7.899699	-0.045948	4.130901
229.342484	5834.467745	7.904704	-0.046013	4.133650
229.527551	5842.494102	7.909709	-0.046053	4.136388
229.513682	5850.471587	7.914714	-0.046055	4.139106
229.706970	5858.574421	7.919718	-0.046096	4.141867
229.799446	5866.467872	7.924723	-0.046118	4.144554
230.003617	5874.552671	7.929728	-0.046162	4.147305
230.193645	5882.583686	7.934733	-0.046202	4.150036
230.248051	5890.605499	7.939738	-0.046217	4.152761
230.578044	5898.655250	7.944742	-0.046284	4.155496
230.747045	5906.631282	7.949747	-0.046320	4.158203
231.125758	5914.631189	7.954752	-0.046396	4.160919
230.996871	5922.648285	7.959757	-0.046377	4.163632
231.018312	5930.664538	7.964762	-0.046386	4.166346
231.416084	5938.690872	7.969766	-0.046465	4.169065
231.627761	5946.727015	7.974771	-0.046509	4.171784
231.849865	5954.725616	7.979776	-0.046556	4.174488
231.868017	5962.783452	7.984781	-0.046564	4.177208
232.012369	5970.758147	7.989786	-0.046596	4.179900
232.361374	5978.780437	7.994790	-0.046666	4.182608
232.240611	5986.774258	7.999795	-0.046649	4.185300
232.552396	5994.816678	8.004800	-0.046712	4.188011
232.665188	6002.833726	8.009805	-0.046738	4.190710
232.870111	6010.935708	8.014810	-0.046781	4.193436
233.171938	6018.963762	8.019814	-0.046842	4.196137
233.266532	6026.903231	8.024819	-0.046865	4.198804
233.429953	6034.894020	8.029824	-0.046900	4.201488
233.698842	6042.871800	8.034829	-0.046955	4.204166
234.184636	6050.899301	8.039834	-0.047051	4.206862
234.246597	6058.888350	8.044838	-0.047067	4.209538
234.272913	6066.948918	8.049843	-0.047077	4.212236
234.609629	6074.986550	8.054848	-0.047145	4.214928
234.663620	6083.007190	8.059853	-0.047160	4.217610
234.614308	6090.991199	8.064858	-0.047156	4.220277
234.943627	6099.046575	8.069862	-0.047222	4.222970
235.243755	6107.036028	8.074867	-0.047283	4.225638
235.359607	6115.024854	8.079872	-0.047310	4.228303
235.619054	6123.080173	8.084877	-0.047363	4.230990
235.762754	6131.129087	8.089882	-0.047395	4.233672
235.973203	6139.164351	8.094886	-0.047439	4.236348
236.241410	6147.119562	8.099891	-0.047494	4.238997
236.555346	6155.146210	8.104896	-0.047558	4.241667
236.721180	6163.143697	8.109901	-0.047593	4.244326
236.734847	6171.180653	8.114906	-0.047601	4.246994
236.833721	6179.207119	8.119910	-0.047625	4.249657
237.092535	6187.204092	8.124915	-0.047678	4.252311
237.201100	6195.268746	8.129920	-0.047703	4.254984
237.480111	6203.303684	8.134925	-0.047760	4.257647
237.645987	6211.274175	8.139930	-0.047796	4.260286
237.779786	6219.314760	8.144934	-0.047826	4.262946
237.744679	6227.327151	8.149939	-0.047824	4.265594
237.957325	6235.363463	8.154944	-0.047869	4.268250
238.152497	6243.392090	8.159949	-0.047910	4.270902
238.255339	6251.422528	8.164954	-0.047935	4.273552
238.623202	6259.506062	8.169958	-0.048008	4.276220
238.748435	6267.441808	8.174963	-0.048036	4.278836
238.979786	6275.455630	8.179968	-0.048085	4.281476
239.094102	6283.456592	8.184973	-0.048111	4.284110
239.298314	6291.454568	8.189978	-0.048154	4.286742
239.370009	6299.484617	8.194982	-0.048172	4.289382
239.309233	6307.547656	8.199987	-0.048166	4.292029
239.677225	6315.564195	8.204992	-0.048240	4.294664
240.126681	6323.577161	8.209997	-0.048328	4.297296
240.117841	6331.547264	8.215002	-0.048332	4.299909
240.285198	6339.603772	8.220006	-0.048368	4.302550
240.583350	6347.551551	8.225011	-0.048428	4.305154
240.657791	6355.612627	8.230016	-0.048447	4.307793
240.828889	6363.618166	8.235021	-0.048484	4.310412
240.991758	6371.691907	8.240026	-0.048520	4.313052
241.231212	6379.688589	8.245030	-0.048569	4.315666
241.321156	6387.684071	8.250035	-0.048591	4.318276
241.448942	6395.698894	8.255040	-0.048620	4.320892
241.821920	6403.713125	8.260045	-0.048694	4.323508
241.776326	6411.697597	8.265050	-0.048691	4.326109
241.972581	6419.761126	8.270054	-0.048732	4.328736
242.108224	6427.754196	8.275059	-0.048763	4.331338
242.358037	6435.785186	8.280064	-0.048814	4.333952
242.363174	6443.834076	8.285069	-0.048820	4.336568
242.480763	6451.805648	8.290074	-0.048847	4.339159
242.726178	6459.858220	8.295078	-0.048898	4.341774
242.847596	6467.821130	8.300083	-0.048925	4.344359
243.083980	6475.849059	8.305088	-0.048975	4.346964
243.303178	6483.891895	8.310093	-0.049020	4.349571
243.361725	6491.890847	8.315098	-0.049036	4.352162
243.693887	6500.031889	8.320102	-0.049103	4.354799
243.980940	6508.014780	8.325107	-0.049162	4.357384
244.310087	6515.954365	8.330112	-0.049228	4.359952
244.145541	6524.002178	8.335117	-0.049202	4.362551
244.303731	6531.908248	8.340122	-0.049237	4.365105
244.688472	6539.989841	8.345126	-0.049314	4.367716
245.077308	6547.994045	8.350131	-0.049391	4.370299
245.298722	6556.010165	8.355136	-0.049437	4.372884
245.275781	6564.064746	8.360141	-0.049438	4.375479
245.615466	6572.069910	8.365146	-0.049506	4.378058
245.636033	6580.104180	8.370150	-0.049515	4.380643
246.049003	6588.076910	8.375155	-0.049597	4.383209
246.097222	6596.077492	8.380160	-0.049611	4.385780
246.309890	6604.137274	8.385165	-0.049656	4.388370
246.403670	6612.122248	8.390170	-0.049678	4.390933
246.669341	6620.203409	8.395174	-0.049733	4.393527
246.687310	6628.186520	8.400179	-0.049741	4.396086
246.645198	6636.201623	8.405184	-0.049738	4.398654
246.859133	6644.251279	8.410189	-0.049783	4.401233
246.953759	6652.181827	8.415194	-0.049806	4.403772
246.920697	6660.268456	8.420198	-0.049805	4.406358
247.063665	6668.227071	8.425203	-0.049836	4.408903
247.324873	6676.318487	8.430208	-0.049890	4.411489
247.474187	6684.327505	8.435213	-0.049923	4.414047
247.531267	6692.356362	8.440218	-0.049939	4.416609
247.933848	6700.348408	8.445222	-0.050019	4.419160
247.974688	6708.361465	8.450227	-0.050031	4.421714
247.991344	6716.345224	8.455232	-0.050039	4.424257
248.445198	6724.448817	8.460237	-0.050129	4.426839
248.517584	6732.423471	8.465242	-0.050147	4.429376
248.440219	6740.503084	8.470246	-0.050138	4.431945
248.731890	6748.521237	8.475251	-0.050197	4.434495
248.877962	6756.528451	8.480256	-0.050230	4.437038
249.078916	6764.469722	8.485261	-0.050272	4.439560
248.956866	6772.486895	8.490266	-0.050254	4.442103
249.461064	6780.518014	8.495270	-0.050353	4.444651
249.729360	6788.567886	8.500275	-0.050408	4.447203
249.631030	6796.529607	8.505280	-0.050395	4.449724
249.883862	6804.603823	8.510285	-0.050447	4.452281
250.011442	6812.587608	8.515290	-0.050476	4.454807
250.371844	6820.662012	8.520294	-0.050548	4.457361
250.613967	6828.569670	8.525299	-0.050598	4.459861
250.862757	6836.631115	8.530304	-0.050649	4.462407
250.969311	6844.641550	8.535309	-0.050674	4.464936
251.031716	6852.675897	8.540314	-0.050691	4.467470
251.168458	6860.684275	8.545318	-0.050721	4.469995
251.354804	6868.719487	8.550323	-0.050761	4.472527
251.441440	6876.724723	8.555328	-0.050782	4.475048
251.514170	6884.803136	8.560333	-0.050801	4.477591
251.673951	6892.688664	8.565338	-0.050836	4.480072
251.851421	6900.752300	8.570343	-0.050874	4.482607
251.916891	6908.734248	8.575347	-0.050891	4.485115
252.100297	6916.801073	8.580352	-0.050930	4.487649
252.490809	6924.820749	8.585357	-0.051008	4.490166
252.455081	6932.808359	8.590362	-0.051006	4.492672
252.949605	6940.864172	8.595367	-0.051103	4.495198
252.815372	6948.866718	8.600371	-0.051083	4.497705
252.934961	6956.865408	8.605376	-0.051111	4.500210
253.159395	6964.939535	8.610381	-0.051158	4.502737
253.324480	6972.859046	8.615386	-0.051193	4.505214
253.587357	6980.915038	8.620391	-0.051247	4.507733
253.602951	6988.962690	8.625395	-0.051255	4.510247
253.795169	6996.989421	8.630400	-0.051296	4.512754
254.049068	7005.043230	8.635405	-0.051348	4.515268
254.085294	7012.997163	8.640410	-0.051360	4.517748
254.456698	7020.997070	8.645415	-0.051434	4.520243
254.584210	7029.030387	8.650419	-0.051463	4.522746
254.854280	7036.969913	8.655424	-0.051518	4.525218
255.035396	7045.039950	8.660429	-0.051557	4.527730
255.078139	7053.003011	8.665434	-0.051570	4.530207
255.222737	7061.057198	8.670439	-0.051602	4.532711
255.248033	7069.117659	8.675443	-0.051612	4.535215
255.638385	7077.107950	8.680448	-0.051690	4.537696
255.792455	7085.113228	8.685453	-0.051723	4.540181
255.791755	7093.063429	8.690458	-0.051728	4.542647
256.134474	7101.114791	8.695463	-0.051797	4.545143
256.250829	7109.139670	8.700467	-0.051824	4.547629
256.389066	7117.154761	8.705472	-0.051855	4.550111
256.710406	7125.259163	8.710477	-0.051919	4.552620
256.821045	7133.232860	8.715482	-0.051945	4.555086
256.972086	7141.212766	8.720487	-0.051978	4.557553
257.129086	7149.204112	8.725491	-0.052012	4.560022
257.294793	7157.260501	8.730496	-0.052048	4.562510
257.353204	7165.230716	8.735501	-0.052064	4.564970
257.581062	7173.269417	8.740506	-0.052112	4.567450
257.734332	7181.271317	8.745511	-0.052145	4.569917
257.925300	7189.348429	8.750515	-0.052186	4.572406
258.076096	7197.368292	8.755520	-0.052219	4.574876
258.364424	7205.458098	8.760525	-0.052278	4.577366
258.355161	7213.362400	8.765530	-0.052281	4.579797
258.444040	7221.430123	8.770535	-0.052303	4.582278
258.618905	7229.392294	8.775539	-0.052340	4.584724
258.877739	7237.435888	8.780544	-0.052393	4.587195
258.914760	7245.461990	8.785549	-0.052405	4.589658
258.921875	7253.522001	8.790554	-0.052412	4.592131
259.340994	7261.557181	8.795559	-0.052495	4.594595
259.444404	7269.567743	8.800563	-0.052519	4.597050
259.636583	7277.463231	8.805568	-0.052560	4.599468
259.666923	7285.579394	8.810573	-0.052571	4.601953
259.783235	7293.474317	8.815578	-0.052597	4.604368
259.890248	7301.548074	8.820583	-0.052622	4.606837
260.043474	7309.547513	8.825587	-0.052656	4.609282
260.253361	7317.586012	8.830592	-0.052700	4.611737
260.429366	7325.679008	8.835597	-0.052738	4.614208
260.706201	7333.661805	8.840602	-0.052794	4.616644
260.817054	7341.619183	8.845607	-0.052820	4.619070
260.917670	7349.671974	8.850611	-0.052844	4.621525
260.917289	7357.635739	8.855616	-0.052849	4.623951
261.070900	7365.719728	8.860621	-0.052882	4.626412
261.156100	7373.685899	8.865626	-0.052903	4.628837
261.740129	7381.730860	8.870631	-0.053017	4.631283
261.654757	7389.755681	8.875635	-0.053006	4.633723
261.903400	7397.791437	8.880640	-0.053057	4.636164
262.178217	7405.782221	8.885645	-0.053114	4.638591
262.095722	7413.763183	8.890650	-0.053103	4.641013
262.326913	7421.807683	8.895655	-0.053151	4.643453
262.283076	7429.821842	8.900659	-0.053148	4.645883
262.542573	7437.848209	8.905664	-0.053202	4.648315
262.567692	7445.861721	8.910669	-0.053211	4.650742
262.743320	7453.830378	8.915674	-0.053249	4.653154
262.926430	7461.862102	8.920679	-0.053288	4.655584
262.996240	7469.891514	8.925683	-0.053306	4.658012
263.109759	7477.888112	8.930688	-0.053332	4.660429
263.484439	7485.925062	8.935693	-0.053407	4.662856
263.620991	7493.875407	8.940698	-0.053438	4.665256
263.631778	7501.956664	8.945703	-0.053445	4.667695
263.724804	7509.977291	8.950707	-0.053467	4.670114
263.785348	7518.019582	8.955712	-0.053483	4.672538
264.111538	7526.107780	8.960717	-0.053549	4.674975
264.114753	7534.054568	8.965722	-0.053555	4.677368
264.404767	7541.992399	8.970727	-0.053614	4.679756
264.705860	7550.020626	8.975731	-0.053675	4.682171
264.572757	7557.976953	8.980736	-0.053655	4.684563
265.055670	7566.079073	8.985741	-0.053750	4.686997
265.137434	7574.024125	8.990746	-0.053770	4.689383
265.323198	7582.113299	8.995751	-0.053810	4.691811
265.358365	7590.145418	9.000755	-0.053822	4.694221
265.602268	7598.150773	9.005760	-0.053872	4.696621
265.948488	7606.107879	9.010765	-0.053941	4.699006
266.068326	7614.147860	9.015770	-0.053969	4.701414
266.403766	7622.168528	9.020775	-0.054036	4.703815
266.563964	7630.174404	9.025779	-0.054071	4.706210
266.498392	7638.193167	9.030784	-0.054064	4.708609
266.699727	7646.227466	9.035789	-0.054106	4.711010
266.752331	7654.217741	9.040794	-0.054121	4.713398
266.797294	7662.272679	9.045799	-0.054135	4.715803
266.909901	7670.297794	9.050803	-0.054161	4.718198
267.203717	7678.234376	9.055808	-0.054220	4.720566
267.367062	7686.359288	9.060813	-0.054256	4.722988
267.344703	7694.269898	9.065818	-0.054257	4.725346
267.750865	7702.346649	9.070823	-0.054337	4.727751
267.867075	7710.352613	9.075827	-0.054364	4.730134
267.885494	7718.401615	9.080832	-0.054373	4.732529
268.206215	7726.420889	9.085837	-0.054437	4.734913
268.192789	7734.451541	9.090842	-0.054440	4.737301
268.260574	7742.400884	9.095847	-0.054457	4.739663
268.414066	7750.481286	9.100851	-0.054491	4.742062
268.617942	7758.395941	9.105856	-0.054534	4.744410
268.773666	7766.489871	9.110861	-0.054568	4.746811
268.909666	7774.485601	9.115866	-0.054598	4.749182
268.973281	7782.488800	9.120871	-0.054615	4.751554
269.192536	7790.620063	9.125875	-0.054661	4.753962
269.370330	7798.538852	9.130880	-0.054699	4.756306
269.679183	7806.550729	9.135885	-0.054762	4.758676
269.739632	7814.515225	9.140890	-0.054778	4.761031
269.811656	7822.548268	9.145895	-0.054797	4.763406
269.802671	7830.574855	9.150899	-0.054800	4.765777
270.222253	7838.552605	9.155904	-0.054883	4.768132
270.329265	7846.641608	9.160909	-0.054908	4.770519
270.318769	7854.606197	9.165914	-0.054911	4.772869
270.568346	7862.659632	9.170919	-0.054963	4.775243
270.793843	7870.646934	9.175923	-0.055010	4.777597
270.938511	7878.613867	9.180928	-0.055042	4.779943
271.282840	7886.751870	9.185933	-0.055111	4.782338
271.331353	7894.645973	9.190938	-0.055125	4.784661
271.428617	7902.720843	9.195943	-0.055148	4.787036
271.684188	7910.708543	9.200947	-0.055201	4.789384
272.076470	7918.784053	9.205952	-0.055279	4.791755
272.261798	7926.847952	9.210957	-0.055318	4.794123
272.071181	7934.807193	9.215962	-0.055288	4.796460
272.190718	7942.761050	9.220967	-0.055315	4.798794
272.372636	7950.818796	9.225971	-0.055354	4.801156
272.449890	7958.772457	9.230976	-0.055373	4.803487
272.826109	7966.856160	9.235981	-0.055448	4.805854
272.725136	7974.787212	9.240986	-0.055435	4.808177
272.991075	7982.874066	9.245991	-0.055489	4.810543
272.991233	7990.399293	9.250995	-0.055494	4.812745
273.198469	7995.085777	9.256000	-0.055535	4.814114
273.507780	7997.704638	9.261005	-0.055595	4.814878
273.422196	7999.075458	9.266010	-0.055579	4.815280
273.722645	7999.533151	9.271015	-0.055635	4.815412
273.891322	8000.490679	9.276019	-0.055667	4.815691
273.658191	8000.461219	9.281024	-0.055624	4.815684
273.935494	8000.473210	9.286029	-0.055675	4.815686
274.102557	8000.454563	9.291034	-0.055706	4.815680
274.058814	8000.327804	9.296039	-0.055698	4.815643
274.010421	8000.504289	9.301043	-0.055688	4.815695
274.208348	8000.462650	9.306048	-0.055725	4.815681
274.298033	8000.463031	9.311053	-0.055742	4.815681
274.113516	8000.518740	9.316058	-0.055707	4.815698
274.180807	8000.353210	9.321063	-0.055719	4.815650
274.248981	8000.496356	9.326067	-0.055732	4.815691
274.225777	8000.489551	9.331072	-0.055727	4.815689
274.316828	8000.473934	9.336077	-0.055744	4.815684
274.495916	8000.470437	9.341082	-0.055777	4.815682
274.830497	8000.382969	9.346087	-0.055839	4.815655
274.690586	8000.396686	9.351091	-0.055813	4.815660
274.749509	8000.458511	9.356096	-0.055824	4.815678
275.029735	8000.496186	9.361101	-0.055876	4.815687
274.430563	8000.436175	9.366106	-0.055764	4.815673
274.574790	8000.272970	9.371111	-0.055791	4.815624
274.762257	8000.412726	9.376115	-0.055825	4.815664
274.660639	8000.481539	9.381120	-0.055806	4.815685
274.628557	8000.413711	9.386125	-0.055800	4.815665
274.811133	8000.386773	9.391130	-0.055834	4.815656
274.704593	8000.364722	9.396135	-0.055814	4.815651
274.562825	8000.362388	9.401139	-0.055787	4.815651
274.698180	8000.570717	9.406144	-0.055813	4.815711
274.947037	8000.498937	9.411149	-0.055859	4.815689
274.860639	8000.478282	9.416154	-0.055842	4.815683
275.047346	8000.468502	9.421159	-0.055877	4.815679
275.254992	8000.397116	9.426163	-0.055915	4.815657
275.094202	8000.485255	9.431168	-0.055885	4.815684
275.252118	8000.332952	9.436173	-0.055914	4.815639
275.188261	8000.451513	9.441178	-0.055902	4.815674
275.232453	8000.380659	9.446183	-0.055910	4.815653
275.122059	8000.501664	9.451187	-0.055890	4.815689
275.337766	8000.402640	9.456192	-0.055930	4.815659
275.368778	8000.422356	9.461197	-0.055935	4.815664
275.216637	8000.517045	9.466202	-0.055907	4.815693
275.211707	8000.386644	9.471207	-0.055906	4.815655
275.279290	8000.466768	9.476211	-0.055918	4.815678
275.059007	8000.479170	9.481216	-0.055877	4.815682
275.124838	8000.505863	9.486221	-0.055889	4.815690
275.119350	8000.474783	9.491226	-0.055888	4.815681
275.322270	8000.481289	9.496231	-0.055925	4.815682
275.336983	8000.397135	9.501235	-0.055928	4.815657
275.105316	8000.436053	9.506240	-0.055884	4.815670
275.443613	8000.402049	9.511245	-0.055947	4.815658
275.277453	8000.422813	9.516250	-0.055916	4.815665
275.521635	8000.256967	9.521255	-0.055961	4.815615
275.423075	8000.417684	9.526259	-0.055943	4.815663
275.450547	8000.483268	9.531264	-0.055948	4.815682
275.348976	8000.388669	9.536269	-0.055929	4.815655
275.531608	8000.487764	9.541274	-0.055962	4.815683
275.409384	8000.470796	9.546279	-0.055939	4.815678
275.211615	8000.495314	9.551283	-0.055902	4.815686
275.044635	8000.488295	9.556288	-0.055871	4.815685
275.399753	8000.251636	9.561293	-0.055937	4.815614
275.401718	8000.494100	9.566298	-0.055937	4.815685
275.162150	8000.477349	9.571303	-0.055893	4.815681
275.371885	8000.512804	9.576307	-0.055931	4.815691
275.499428	8000.393113	9.581312	-0.055955	4.815655
275.469404	8000.231329	9.586317	-0.055949	4.815608
275.404398	8000.513285	9.591322	-0.055937	4.815691
275.572452	8000.249001	9.596327	-0.055968	4.815613
275.630758	8000.322565	9.601331	-0.055979	4.815634
275.512584	8000.480826	9.606336	-0.055956	4.815681
275.874678	8000.264572	9.611341	-0.056024	4.815616
275.655559	8000.483130	9.616346	-0.055983	4.815681
275.660969	8000.407369	9.621351	-0.055983	4.815659
275.818879	8000.354395	9.626355	-0.056013	4.815642
275.689570	8000.392850	9.631360	-0.055988	4.815654
275.591847	8000.486293	9.636365	-0.055970	4.815682
275.593339	8000.422216	9.641370	-0.055970	4.815663
275.579412	8000.294872	9.646375	-0.055967	4.815626
275.705601	8000.397317	9.651379	-0.055991	4.815656
275.611725	8000.387220	9.656384	-0.055973	4.815653
275.793855	8000.382705	9.661389	-0.056007	4.815651
275.874477	8000.405368	9.666394	-0.056021	4.815657
275.662958	8000.316447	9.671399	-0.055982	4.815632
275.693458	8000.497432	9.676403	-0.055987	4.815685
275.737871	8000.371042	9.681408	-0.055995	4.815648
275.916143	8000.361123	9.686413	-0.056028	4.815644
275.608565	8000.508810	9.691418	-0.055971	4.815689
275.863452	8000.480920	9.696423	-0.056018	4.815679
275.837896	8000.277552	9.701427	-0.056013	4.815620
275.788122	8000.526649	9.706432	-0.056004	4.815693
275.882462	8000.230184	9.711437	-0.056021	4.815606
275.896735	8000.526256	9.716442	-0.056024	4.815692
275.871857	8000.331443	9.721447	-0.056019	4.815636
275.988548	8000.400623	9.726451	-0.056040	4.815655
275.965996	8000.469662	9.731456	-0.056036	4.815675
276.124742	8000.274648	9.736461	-0.056065	4.815618
275.863005	8000.379294	9.741466	-0.056016	4.815650
275.802392	8000.282160	9.746471	-0.056005	4.815621
275.928958	8000.157113	9.751475	-0.056028	4.815584
275.906934	8000.389574	9.756480	-0.056024	4.815652
275.941482	8000.401871	9.761485	-0.056030	4.815656
276.045374	8000.422779	9.766490	-0.056049	4.815661
276.038030	8000.360694	9.771495	-0.056048	4.815643
276.138003	8000.318521	9.776499	-0.056066	4.815631
276.208838	8000.457444	9.781504	-0.056079	4.815671
276.128978	8000.425147	9.786509	-0.056064	4.815662
275.892509	8000.428739	9.791514	-0.056020	4.815664
276.056672	8000.445292	9.796519	-0.056050	4.815668
276.097231	8000.447007	9.801523	-0.056058	4.815668
275.868715	8000.476363	9.806528	-0.056015	4.815678
276.131453	8000.480643	9.811533	-0.056064	4.815678
276.034803	8000.402144	9.816538	-0.056046	4.815656
276.105953	8000.391542	9.821543	-0.056059	4.815652
276.108003	8000.489822	9.826547	-0.056059	4.815681
275.950094	8000.510720	9.831552	-0.056029	4.815688
275.974463	8000.265445	9.836557	-0.056033	4.815616
276.040594	8000.363704	9.841562	-0.056046	4.815644
276.177508	8000.350973	9.846567	-0.056071	4.815640
276.091312	8000.295075	9.851571	-0.056055	4.815624
276.182637	8000.522984	9.856576	-0.056072	4.815690
276.198420	8000.223096	9.861581	-0.056074	4.815602
276.260357	8000.524222	9.866586	-0.056086	4.815690
276.102138	8000.461804	9.871591	-0.056056	4.815673
276.146109	8000.326860	9.876595	-0.056064	4.815633
276.239593	8000.417023	9.881600	-0.056081	4.815659
276.281728	8000.372836	9.886605	-0.056089	4.815646
275.952189	8000.395199	9.891610	-0.056027	4.815654
276.058304	8000.559266	9.896615	-0.056047	4.815701
276.400332	8000.395019	9.901619	-0.056110	4.815652
276.260724	8000.456803	9.906624	-0.056084	4.815670
276.247452	8000.396757	9.911629	-0.056081	4.815653
276.187714	8000.408580	9.916634	-0.056070	4.815657
276.232944	8000.370852	9.921639	-0.056078	4.815646
276.215320	8000.506193	9.926643	-0.056075	4.815685
276.163452	8000.350456	9.931648	-0.056065	4.815640
276.313884	8000.278134	9.936653	-0.056093	4.815618
276.179815	8000.381664	9.941658	-0.056068	4.815649
276.188066	8000.467229	9.946663	-0.056069	4.815674
276.134316	8000.370206	9.951667	-0.056059	4.815646
276.137095	8000.394800	9.956672	-0.056059	4.815653
276.216361	8000.258298	9.961677	-0.056074	4.815613
276.357525	8000.483818	9.966682	-0.056100	4.815678
276.439938	8000.458448	9.971687	-0.056115	4.815670
276.294649	8000.429352	9.976691	-0.056088	4.815662
276.263170	8000.383961	9.981696	-0.056082	4.815649
276.366976	8000.279902	9.986701	-0.056101	4.815618
276.262839	8000.461891	9.991706	-0.056081	4.815672
276.370914	8000.410238	9.996711	-0.056101	4.815656
276.464611	8000.402141	10.001715	-0.056118	4.815654
276.380803	8000.419979	10.006720	-0.056103	4.815659
276.523851	8000.383851	10.011725	-0.056129	4.815648
276.632881	8000.508448	10.016730	-0.056149	4.815684
276.628920	8000.273387	10.021735	-0.056148	4.815615
276.567951	8000.404815	10.026739	-0.056137	4.815654
276.360879	8000.482586	10.031744	-0.056098	4.815678
276.270106	8000.461858	10.036749	-0.056081	4.815672
276.207427	8000.475769	10.041754	-0.056069	4.815676
276.357500	8000.476071	10.046759	-0.056097	4.815676
276.495308	8000.365092	10.051763	-0.056122	4.815643
276.537806	8000.501417	10.056768	-0.056130	4.815682
276.466115	8000.403031	10.061773	-0.056116	4.815654
276.469729	8000.391325	10.066778	-0.056117	4.815651
276.398772	8000.457437	10.071783	-0.056104	4.815670
276.519736	8000.323752	10.076787	-0.056126	4.815631
276.459408	8000.451986	10.081792	-0.056114	4.815668
276.475416	8000.297359	10.086797	-0.056117	4.815623
276.395208	8000.401770	10.091802	-0.056102	4.815654
276.368639	8000.398115	10.096807	-0.056097	4.815653
276.414003	8000.419133	10.101811	-0.056105	4.815659
276.395705	8000.440179	10.106816	-0.056102	4.815665
276.391497	8000.380281	10.111821	-0.056101	4.815648
276.383918	8000.497629	10.116826	-0.056099	4.815682
276.516143	8000.499775	10.121831	-0.056124	4.815682
276.604051	8000.401864	10.126835	-0.056140	4.815653
276.340948	8000.544939	10.131840	-0.056091	4.815696
276.576957	8000.304192	10.136845	-0.056134	4.815625
276.467962	8000.504260	10.141850	-0.056114	4.815684
276.359431	8000.347596	10.146855	-0.056093	4.815638
276.542336	8000.376204	10.151859	-0.056127	4.815646
276.595458	8000.396282	10.156864	-0.056137	4.815651
276.710400	8000.298813	10.161869	-0.056158	4.815622
276.470870	8000.338670	10.166874	-0.056113	4.815635
276.717086	8000.318115	10.171879	-0.056159	4.815628
276.640698	8000.431133	10.176883	-0.056145	4.815661
276.514993	8000.353226	10.181888	-0.056121	4.815639
276.884281	8000.200105	10.186893	-0.056189	4.815593
276.686314	8000.408331	10.191898	-0.056152	4.815655
276.403611	8000.208232	10.196903	-0.056099	4.815597
276.478470	8000.335472	10.201907	-0.056113	4.815634
276.663830	8000.381210	10.206912	-0.056148	4.815647
276.430306	8000.314357	10.211917	-0.056104	4.815628
276.222759	8000.482906	10.216922	-0.056065	4.815679
276.447092	8000.322074	10.221927	-0.056107	4.815631
276.452932	8000.243115	10.226931	-0.056108	4.815607
276.293482	8000.300303	10.231936	-0.056078	4.815625
276.334138	8000.289202	10.236941	-0.056085	4.815621
276.349141	8000.399443	10.241946	-0.056088	4.815654
276.300503	8000.308912	10.246951	-0.056078	4.815627
276.504945	8000.269515	10.251955	-0.056116	4.815615
276.606588	8000.483710	10.256960	-0.056135	4.815677
276.761252	8000.324942	10.261965	-0.056164	4.815630
276.744766	8000.397285	10.266970	-0.056160	4.815651
276.768151	8000.320748	10.271975	-0.056165	4.815629
276.693137	8000.408156	10.276979	-0.056150	4.815655
276.425314	8000.425119	10.281984	-0.056100	4.815661
276.663277	8000.314710	10.286989	-0.056144	4.815627
276.731441	8000.490975	10.291994	-0.056157	4.815679
276.612577	8000.442017	10.296999	-0.056135	4.815665
276.468250	8000.572083	10.302003	-0.056108	4.815704
276.455801	8000.463985	10.307008	-0.056105	4.815672
276.499537	8000.373896	10.312013	-0.056113	4.815646
276.515382	8000.572803	10.317018	-0.056116	4.815704
276.581763	8000.464927	10.322023	-0.056128	4.815672
276.669453	8000.369148	10.327027	-0.056144	4.815643
276.510883	8000.437031	10.332032	-0.056114	4.815664
276.487465	8000.304189	10.337037	-0.056110	4.815625
276.651928	8000.519412	10.342042	-0.056140	4.815687
276.510512	8000.439111	10.347047	-0.056114	4.815665
276.446609	8000.391053	10.352051	-0.056102	4.815651
276.575526	8000.492477	10.357056	-0.056126	4.815680
276.731033	8000.370038	10.362061	-0.056154	4.815643
276.624340	8000.496446	10.367066	-0.056134	4.815681
276.737070	8000.387192	10.372071	-0.056155	4.815648
276.710570	8000.506368	10.377075	-0.056150	4.815683
276.644848	8000.468961	10.382080	-0.056137	4.815673
276.757534	8000.365046	10.387085	-0.056158	4.815642
276.627345	8000.400283	10.392090	-0.056134	4.815653
276.595590	8000.389066	10.397095	-0.056128	4.815650
276.726169	8000.397593	10.402099	-0.056152	4.815651
276.621163	8000.408676	10.407104	-0.056132	4.815655
276.643148	8000.387657	10.412109	-0.056136	4.815649
276.604582	8000.495954	10.417114	-0.056129	4.815681
276.788141	8000.277846	10.422119	-0.056162	4.815616
276.777945	8000.341747	10.427123	-0.056160	4.815635
276.672910	8000.406234	10.432128	-0.056141	4.815654
276.877401	8000.375383	10.437133	-0.056179	4.815644
276.947514	8000.383990	10.442138	-0.056191	4.815646
276.839979	8000.481547	10.447143	-0.056171	4.815675
276.837256	8000.386425	10.452147	-0.056171	4.815648
276.720664	8000.369547	10.457152	-0.056149	4.815643
276.874270	8000.430788	10.462157	-0.056177	4.815660
276.827305	8000.423595	10.467162	-0.056168	4.815659
276.782115	8000.485856	10.472167	-0.056160	4.815677
276.942209	8000.369900	10.477171	-0.056189	4.815642
276.732899	8000.443361	10.482176	-0.056150	4.815665
276.838261	8000.261357	10.487181	-0.056169	4.815611
277.114659	8000.412190	10.492186	-0.056221	4.815654
276.805998	8000.188166	10.497191	-0.056163	4.815590
276.675455	8000.212716	10.502195	-0.056138	4.815598
276.827808	8000.527073	10.507200	-0.056167	4.815689
276.994125	8000.257414	10.512205	-0.056197	4.815609
276.958561	8000.391394	10.517210	-0.056191	4.815649
276.640654	8000.481237	10.522215	-0.056131	4.815676
276.917455	8000.367190	10.527219	-0.056183	4.815642
276.650579	8000.405531	10.532224	-0.056133	4.815654
276.653534	8000.379928	10.537229	-0.056133	4.815647
276.716615	8000.399101	10.542234	-0.056145	4.815652
276.763611	8000.455393	10.547239	-0.056153	4.815668
276.779320	8000.386208	10.552243	-0.056156	4.815648
276.803068	8000.392988	10.557248	-0.056160	4.815650
276.842848	8000.347694	10.562253	-0.056167	4.815636
276.772973	8000.389257	10.567258	-0.056154	4.815649
276.639746	8000.379585	10.572263	-0.056129	4.815647
276.870541	8000.191088	10.577267	-0.056172	4.815591
276.829880	8000.389070	10.582272	-0.056164	4.815649
276.915182	8000.279367	10.587277	-0.056180	4.815616
276.785129	8000.306061	10.592282	-0.056155	4.815625
276.766060	8000.307869	10.597287	-0.056152	4.815625
276.661900	8000.309352	10.602291	-0.056132	4.815626
276.749501	8000.351355	10.607296	-0.056148	4.815638
276.973756	8000.362484	10.612301	-0.056190	4.815640
276.978134	8000.417011	10.617306	-0.056190	4.815656
276.790854	8000.303917	10.622311	-0.056155	4.815624
276.866173	8000.374558	10.627315	-0.056169	4.815644
276.759050	8000.489211	10.632320	-0.056149	4.815678
276.768624	8000.286414	10.637325	-0.056151	4.815619
276.860660	8000.326353	10.642330	-0.056168	4.815630
276.791533	8000.311321	10.647335	-0.056154	4.815626
276.729198	8000.346599	10.652339	-0.056143	4.815637
276.764274	8000.372790	10.657344	-0.056149	4.815644
276.857586	8000.272831	10.662349	-0.056166	4.815615
276.882484	8000.467614	10.667354	-0.056171	4.815671
276.725054	8000.426570	10.672359	-0.056141	4.815660
276.931917	8000.309243	10.677363	-0.056179	4.815625
276.740317	8000.435331	10.682368	-0.056144	4.815663
276.872201	8000.400088	10.687373	-0.056168	4.815652
277.041825	8000.391098	10.692378	-0.056199	4.815648
277.078305	8000.495283	10.697383	-0.056206	4.815679
277.009155	8000.404415	10.702387	-0.056193	4.815652
276.775073	8000.384547	10.707392	-0.056149	4.815648
276.767542	8000.375862	10.712397	-0.056148	4.815645
276.650602	8000.383545	10.717402	-0.056126	4.815648
276.784572	8000.478644	10.722407	-0.056150	4.815675
276.863894	8000.363503	10.727411	-0.056165	4.815641
276.759394	8000.387410	10.732416	-0.056145	4.815649
276.819005	8000.387300	10.737421	-0.056156	4.815648
277.045475	8000.296997	10.742426	-0.056198	4.815621
276.912585	8000.445407	10.747431	-0.056173	4.815665
276.779755	8000.412242	10.752435	-0.056148	4.815656
276.814748	8000.387163	10.757440	-0.056155	4.815648
276.836079	8000.366134	10.762445	-0.056158	4.815642
276.748749	8000.461884	10.767450	-0.056142	4.815670
276.803364	8000.407220	10.772455	-0.056152	4.815654
276.899774	8000.394895	10.777459	-0.056170	4.815650
276.919537	8000.492398	10.782464	-0.056173	4.815679
276.643339	8000.447275	10.787469	-0.056122	4.815667
276.608451	8000.417849	10.792474	-0.056115	4.815658
276.751027	8000.389190	10.797479	-0.056141	4.815649
276.765726	8000.376597	10.802483	-0.056144	4.815646
276.730498	8000.511651	10.807488	-0.056137	4.815685
276.736188	8000.273544	10.812493	-0.056138	4.815616
276.707614	8000.333940	10.817498	-0.056132	4.815633
276.468158	8000.315054	10.822503	-0.056088	4.815629
276.788339	8000.352316	10.827507	-0.056147	4.815638
276.721472	8000.477240	10.832512	-0.056134	4.815675
276.729966	8000.358804	10.837517	-0.056136	4.815641
276.891498	8000.348613	10.842522	-0.056166	4.815637
277.056106	8000.335267	10.847527	-0.056196	4.815632
277.096130	8000.385037	10.852531	-0.056203	4.815646
277.048301	8000.489980	10.857536	-0.056194	4.815677
277.265991	8000.340787	10.862541	-0.056235	4.815633
277.304818	8000.388401	10.867546	-0.056242	4.815646
277.166785	8000.381854	10.872551	-0.056216	4.815645
277.226670	8000.356114	10.877555	-0.056227	4.815637
277.111391	8000.427910	10.882560	-0.056205	4.815659
277.062503	8000.386505	10.887565	-0.056196	4.815647
277.050915	8000.406593	10.892570	-0.056193	4.815653
277.121462	8000.388504	10.897575	-0.056206	4.815647
277.172211	8000.233376	10.902579	-0.056216	4.815602
276.805081	8000.509329	10.907584	-0.056147	4.815684
276.934237	8000.355484	10.912589	-0.056171	4.815639
276.987191	8000.423623	10.917594	-0.056181	4.815658
276.861871	8000.347858	10.922599	-0.056157	4.815637
277.085093	8000.407034	10.927603	-0.056198	4.815653
276.942970	8000.319245	10.932608	-0.056172	4.815628
277.039069	8000.283417	10.937613	-0.056189	4.815617
276.997299	8000.304078	10.942618	-0.056181	4.815623
276.951150	8000.236017	10.947623	-0.056173	4.815604
277.079899	8000.392979	10.952627	-0.056197	4.815649
277.033489	8000.511830	10.957632	-0.056188	4.815684
276.848638	8000.236426	10.962637	-0.056153	4.815604
277.085419	8000.463513	10.967642	-0.056197	4.815670
276.927945	8000.442762	10.972647	-0.056167	4.815664
276.940858	8000.289152	10.977651	-0.056170	4.815619
277.032718	8000.371812	10.982656	-0.056187	4.815643
277.203951	8000.434410	10.987661	-0.056218	4.815660
277.191753	8000.411764	10.992666	-0.056216	4.815654
277.065626	8000.529310	10.997671	-0.056192	4.815689
277.231135	8000.303429	11.002675	-0.056223	4.815622
277.260153	8000.354087	11.007680	-0.056228	4.815637
277.197870	8000.389366	11.012685	-0.056216	4.815647
277.116098	8000.386943	11.017690	-0.056201	4.815647
277.139977	8000.378772	11.022695	-0.056205	4.815645
277.325905	8000.239741	11.027699	-0.056239	4.815603
277.121311	8000.455336	11.032704	-0.056201	4.815667
277.076262	8000.417199	11.037709	-0.056193	4.815656
276.852360	8000.355842	11.042714	-0.056151	4.815639
276.863661	8000.393393	11.047719	-0.056153	4.815650
277.232964	8000.393010	11.052723	-0.056221	4.815648
276.904305	8000.508310	11.057728	-0.056160	4.815684
276.997531	8000.477776	11.062733	-0.056177	4.815674
277.159481	8000.377872	11.067738	-0.056207	4.815644
277.200444	8000.368912	11.072743	-0.056214	4.815641
277.065440	8000.403002	11.077747	-0.056189	4.815652
277.192033	8000.464869	11.082752	-0.056212	4.815670
277.165569	8000.304205	11.087757	-0.056207	4.815623
277.146301	8000.265422	11.092762	-0.056203	4.815611
277.155117	8000.301864	11.097767	-0.056205	4.815622
277.494728	8000.408873	11.102771	-0.056268	4.815652
277.087014	8000.416070	11.107776	-0.056192	4.815656
277.059289	8000.353651	11.112781	-0.056187	4.815638
277.261991	8000.272571	11.117786	-0.056224	4.815613
277.090981	8000.249463	11.122791	-0.056192	4.815607
277.102311	8000.181274	11.127795	-0.056194	4.815587
277.318012	8000.443264	11.132800	-0.056234	4.815663
277.225352	8000.280448	11.137805	-0.056216	4.815616
277.117705	8000.499766	11.142810	-0.056196	4.815680
277.185504	8000.375891	11.147815	-0.056209	4.815644
277.045230	8000.351149	11.152819	-0.056182	4.815637
277.121843	8000.396178	11.157824	-0.056196	4.815650
277.133113	8000.225451	11.162829	-0.056198	4.815600
277.260369	8000.315099	11.167834	-0.056222	4.815626
277.203195	8000.410275	11.172839	-0.056211	4.815654
277.209073	8000.275775	11.177843	-0.056212	4.815614
277.205644	8000.375034	11.182848	-0.056211	4.815643
277.203636	8000.188069	11.187853	-0.056210	4.815589
277.336289	8000.367525	11.192858	-0.056235	4.815641
277.145249	8000.415651	11.197863	-0.056199	4.815656
277.285479	8000.256647	11.202867	-0.056225	4.815608
277.168415	8000.374341	11.207872	-0.056203	4.815643
277.219317	8000.130565	11.212877	-0.056212	4.815572
277.227895	8000.407323	11.217882	-0.056214	4.815653
277.072856	8000.266986	11.222887	-0.056185	4.815612
277.218165	8000.198852	11.227891	-0.056212	4.815592
277.122400	8000.399138	11.232896	-0.056194	4.815651
277.223268	8000.385818	11.237901	-0.056212	4.815646
277.294892	8000.232099	11.242906	-0.056225	4.815601
277.155153	8000.219116	11.247911	-0.056199	4.815598
277.397394	8000.315986	11.252915	-0.056244	4.815625
277.399998	8000.413208	11.257920	-0.056244	4.815654
277.256808	8000.323265	11.262925	-0.056218	4.815628
277.235553	8000.358147	11.267930	-0.056213	4.815638
277.441519	8000.370045	11.272935	-0.056252	4.815641
277.412035	8000.256328	11.277939	-0.056246	4.815608
277.251073	8000.386121	11.282944	-0.056216	4.815646
277.461454	8000.124659	11.287949	-0.056255	4.815569
277.363223	8000.348403	11.292954	-0.056236	4.815635
277.313193	8000.318729	11.297959	-0.056227	4.815626
277.474167	8000.146178	11.302963	-0.056256	4.815575
277.406282	8000.255064	11.307968	-0.056244	4.815607
277.373681	8000.358119	11.312973	-0.056237	4.815638
277.401725	8000.215436	11.317978	-0.056242	4.815596
277.222422	8000.345998	11.322983	-0.056209	4.815635
277.367479	8000.140076	11.327987	-0.056235	4.815574
277.343101	8000.416297	11.332992	-0.056231	4.815655
277.381327	8000.216103	11.337997	-0.056238	4.815596
277.265372	8000.324203	11.343002	-0.056216	4.815628
277.216659	8000.329798	11.348007	-0.056207	4.815630
277.338166	8000.205734	11.353011	-0.056229	4.815593
277.437605	8000.428440	11.358016	-0.056248	4.815658
277.298936	8000.326821	11.363021	-0.056222	4.815629
277.439874	8000.362221	11.368026	-0.056248	4.815639
277.429315	8000.402619	11.373031	-0.056245	4.815651
277.294090	8000.387572	11.378035	-0.056220	4.815647
277.282364	8000.439700	11.383040	-0.056218	4.815662
277.352457	8000.274207	11.388045	-0.056230	4.815613
277.285205	8000.359606	11.393050	-0.056218	4.815639
277.174751	8000.430412	11.398055	-0.056197	4.815660
277.424068	8000.309507	11.403059	-0.056243	4.815623
277.390194	8000.394384	11.408064	-0.056237	4.815648
277.415664	8000.388375	11.413069	-0.056241	4.815646
277.600271	8000.245049	11.418074	-0.056275	4.815604
277.501636	8000.404702	11.423079	-0.056257	4.815651
277.554507	8000.316897	11.428083	-0.056267	4.815625
277.346147	8000.373285	11.433088	-0.056228	4.815642
277.571962	8000.335307	11.438093	-0.056269	4.815630
277.616687	8000.404380	11.443098	-0.056278	4.815650
277.322842	8000.221184	11.448103	-0.056223	4.815598
277.287914	8000.308179	11.453107	-0.056216	4.815624
277.317634	8000.143095	11.458112	-0.056221	4.815575
277.364350	8000.376686	11.463117	-0.056230	4.815643
277.170458	8000.296594	11.468122	-0.056194	4.815621
277.246499	8000.400358	11.473127	-0.056208	4.815651
277.379487	8000.177150	11.478131	-0.056232	4.815585
277.411357	8000.341072	11.483136	-0.056238	4.815633
277.446676	8000.327748	11.488141	-0.056244	4.815629
277.428127	8000.151192	11.493146	-0.056240	4.815577
277.221366	8000.289849	11.498151	-0.056202	4.815619
277.457745	8000.115328	11.503155	-0.056246	4.815567
277.439287	8000.294448	11.508160	-0.056242	4.815619
277.597930	8000.211579	11.513165	-0.056271	4.815594
277.473920	8000.322752	11.518170	-0.056248	4.815627
277.402750	8000.345069	11.523175	-0.056235	4.815634
277.551052	8000.200081	11.528179	-0.056262	4.815591
277.480234	8000.323872	11.533184	-0.056249	4.815627
277.509446	8000.393760	11.538189	-0.056254	4.815648
277.601208	8000.227553	11.543194	-0.056271	4.815599
277.394588	8000.280765	11.548199	-0.056232	4.815615
277.269441	8000.245590	11.553203	-0.056209	4.815606
277.375440	8000.368002	11.558208	-0.056228	4.815641
277.465855	8000.369464	11.563213	-0.056245	4.815641
277.343387	8000.257430	11.568218	-0.056222	4.815609
277.244934	8000.230169	11.573223	-0.056203	4.815601
277.470675	8000.228504	11.578227	-0.056245	4.815600
277.496983	8000.357089	11.583232	-0.056250	4.815637
277.487955	8000.327017	11.588237	-0.056248	4.815628
277.771085	8000.223755	11.593242	-0.056301	4.815597
277.651473	8000.231394	11.598247	-0.056278	4.815600
277.798065	8000.185711	11.603251	-0.056305	4.815586
277.609708	8000.223200	11.608256	-0.056270	4.815597
277.498353	8000.409347	11.613261	-0.056249	4.815652
277.319445	8000.359406	11.618266	-0.056216	4.815639
277.218051	8000.371616	11.623271	-0.056196	4.815643
277.424338	8000.276709	11.628275	-0.056235	4.815614
277.420120	8000.362071	11.633280	-0.056234	4.815639
277.540777	8000.383254	11.638285	-0.056256	4.815645
277.638373	8000.107129	11.643290	-0.056274	4.815563
277.245690	8000.355962	11.648295	-0.056201	4.815638
277.419234	8000.199639	11.653299	-0.056233	4.815592
277.452211	8000.294154	11.658304	-0.056239	4.815619
277.498287	8000.284209	11.663309	-0.056247	4.815616
277.543703	8000.320183	11.668314	-0.056255	4.815626
277.406861	8000.347834	11.673319	-0.056230	4.815635
277.682046	8000.373682	11.678323	-0.056281	4.815641
277.552461	8000.423881	11.683328	-0.056256	4.815656
277.643418	8000.322815	11.688333	-0.056273	4.815626
277.778502	8000.241696	11.693338	-0.056298	4.815602
277.463189	8000.398872	11.698343	-0.056239	4.815650
277.749059	8000.358672	11.703347	-0.056292	4.815636
277.656770	8000.381711	11.708352	-0.056275	4.815644
277.516174	8000.493681	11.713357	-0.056249	4.815677
277.546111	8000.296555	11.718362	-0.056254	4.815619
277.457453	8000.285475	11.723367	-0.056237	4.815616
277.565607	8000.263730	11.728371	-0.056257	4.815610
277.499979	8000.281865	11.733376	-0.056245	4.815615
277.348616	8000.333844	11.738381	-0.056216	4.815631
277.538856	8000.325191	11.743386	-0.056252	4.815628
277.401430	8000.384875	11.748391	-0.056226	4.815646
277.435686	8000.181413	11.753395	-0.056232	4.815586
277.484816	8000.496220	11.758400	-0.056241	4.815678
277.537661	8000.483183	11.763405	-0.056251	4.815674
277.560204	8000.332932	11.768410	-0.056255	4.815630
277.358285	8000.472737	11.773415	-0.056217	4.815672
277.607314	8000.314444	11.778419	-0.056263	4.815624
277.478448	8000.496032	11.783424	-0.056239	4.815678
277.452844	8000.261682	11.788429	-0.056234	4.815610
277.555347	8000.372288	11.793434	-0.056253	4.815641
277.575042	8000.414250	11.798439	-0.056256	4.815654
277.651726	8000.169825	11.803443	-0.056270	4.815582
277.546526	8000.408409	11.808448	-0.056251	4.815652
277.494430	8000.183240	11.813453	-0.056241	4.815587
277.497917	8000.334949	11.818458	-0.056241	4.815631
277.339167	8000.379331	11.823463	-0.056211	4.815645
277.829050	8000.374513	11.828467	-0.056302	4.815641
277.710755	8000.275363	11.833472	-0.056280	4.815612
277.697738	8000.374466	11.838477	-0.056278	4.815641
277.783303	8000.339534	11.843482	-0.056293	4.815631
277.750024	8000.262069	11.848487	-0.056287	4.815608
277.708006	8000.285931	11.853491	-0.056279	4.815616
277.520095	8000.278568	11.858496	-0.056244	4.815614
277.692218	8000.206600	11.863501	-0.056275	4.815592
277.761515	8000.171402	11.868506	-0.056288	4.815582
277.651356	8000.277460	11.873511	-0.056268	4.815613
277.643312	8000.265563	11.878515	-0.056266	4.815610
277.794119	8000.370551	11.883520	-0.056294	4.815640
277.532613	8000.244492	11.888525	-0.056245	4.815604
277.590604	8000.347961	11.893530	-0.056255	4.815634
277.733200	8000.306485	11.898535	-0.056282	4.815621
277.704266	8000.357264	11.903539	-0.056276	4.815636
277.781055	8000.299758	11.908544	-0.056290	4.815619
277.901548	8000.338028	11.913549	-0.056313	4.815630
277.689487	8000.374061	11.918554	-0.056273	4.815641
277.761684	8000.303663	11.923559	-0.056286	4.815621
277.663324	8000.130074	11.928563	-0.056268	4.815570
277.690812	8000.423165	11.933568	-0.056273	4.815656
277.733695	8000.404624	11.938573	-0.056280	4.815650
277.738311	8000.308553	11.943578	-0.056281	4.815622
277.621958	8000.200891	11.948583	-0.056259	4.815591
277.600157	8000.174884	11.953587	-0.056255	4.815584
277.670278	8000.248644	11.958592	-0.056268	4.815605
277.828834	8000.190340	11.963597	-0.056297	4.815587
277.805634	8000.219850	11.968602	-0.056293	4.815596
277.611818	8000.275408	11.973607	-0.056256	4.815613
277.746557	8000.135539	11.978611	-0.056281	4.815572
277.741815	8000.295658	11.983616	-0.056280	4.815618
277.594842	8000.178951	11.988621	-0.056253	4.815585
277.638686	8000.177515	11.993626	-0.056260	4.815584
277.612365	8000.394959	11.998631	-0.056256	4.815648
277.883307	8000.375878	12.003635	-0.056306	4.815641
277.731312	8000.458822	12.008640	-0.056277	4.815666
277.741347	8000.438675	12.013645	-0.056279	4.815660
277.697260	8000.290539	12.018650	-0.056270	4.815617
277.797076	8000.353037	12.023655	-0.056289	4.815635
277.740838	8000.368121	12.028659	-0.056278	4.815640
277.827795	8000.377004	12.033664	-0.056294	4.815642
277.629353	8000.361991	12.038669	-0.056257	4.815638
277.571382	8000.378115	12.043674	-0.056246	4.815643
277.558136	8000.437695	12.048679	-0.056244	4.815661
277.735252	8000.436304	12.053683	-0.056276	4.815660
277.680135	8000.243127	12.058688	-0.056266	4.815603
277.638223	8000.341758	12.063693	-0.056258	4.815632
277.923277	8000.272706	12.068698	-0.056311	4.815611
277.773138	8000.341795	12.073703	-0.056283	4.815632
277.770580	8000.184726	12.078707	-0.056282	4.815586
277.977183	8000.373939	12.083712	-0.056320	4.815640
277.705236	8000.394039	12.088717	-0.056269	4.815647
277.523739	8000.350464	12.093722	-0.056235	4.815636
277.623541	8000.432188	12.098727	-0.056254	4.815659
277.640634	8000.199606	12.103731	-0.056257	4.815591
277.516202	8000.341746	12.108736	-0.056233	4.815633
277.511268	8000.317082	12.113741	-0.056232	4.815626
277.706347	8000.310644	12.118746	-0.056268	4.815623
277.413121	8000.437205	12.123751	-0.056214	4.815661
277.418849	8000.218323	12.128755	-0.056214	4.815597
277.536539	8000.383650	12.133760	-0.056236	4.815645
277.492033	8000.250461	12.138765	-0.056228	4.815606
277.521611	8000.282971	12.143770	-0.056233	4.815616
277.771842	8000.357543	12.148775	-0.056279	4.815636
277.788154	8000.348180	12.153779	-0.056282	4.815634
277.692430	8000.387184	12.158784	-0.056264	4.815646
277.486472	8000.169111	12.163789	-0.056226	4.815583
277.791230	8000.286229	12.168794	-0.056282	4.815616
277.705536	8000.416187	12.173799	-0.056266	4.815654
277.594803	8000.207148	12.178803	-0.056245	4.815593
277.697374	8000.350865	12.183808	-0.056264	4.815635
277.734344	8000.270278	12.188813	-0.056271	4.815611
277.680658	8000.237340	12.193818	-0.056261	4.815602
277.641493	8000.404374	12.198823	-0.056253	4.815651
277.678305	8000.278923	12.203827	-0.056260	4.815614
277.609620	8000.302349	12.208832	-0.056247	4.815621
277.555402	8000.308922	12.213837	-0.056237	4.815623
277.869666	8000.337545	12.218842	-0.056295	4.815630
277.600544	8000.298946	12.223847	-0.056245	4.815620
277.581976	8000.232403	12.228851	-0.056241	4.815601
277.720335	8000.218628	12.233856	-0.056266	4.815596
277.837775	8000.350841	12.238861	-0.056288	4.815634
277.753079	8000.240492	12.243866	-0.056272	4.815602
277.666442	8000.385387	12.248871	-0.056256	4.815645
277.720331	8000.351005	12.253875	-0.056266	4.815635
277.771851	8000.215114	12.258880	-0.056275	4.815595
277.629541	8000.322783	12.263885	-0.056248	4.815627
277.728006	8000.254951	12.268890	-0.056267	4.815607
277.593795	8000.406544	12.273895	-0.056242	4.815652
277.553185	8000.327892	12.278899	-0.056234	4.815629
277.721592	8000.374422	12.283904	-0.056265	4.815642
277.713158	8000.249300	12.288909	-0.056263	4.815605
277.743007	8000.324538	12.293914	-0.056268	4.815627
277.750928	8000.272314	12.298919	-0.056270	4.815612
277.949394	8000.331086	12.303923	-0.056307	4.815628
277.699468	8000.377180	12.308928	-0.056260	4.815643
277.716629	8000.394534	12.313933	-0.056263	4.815648
277.991025	8000.384054	12.318938	-0.056314	4.815643
277.951099	8000.349204	12.323943	-0.056306	4.815633
277.825435	8000.207210	12.328947	-0.056282	4.815592
277.694588	8000.206121	12.333952	-0.056258	4.815593
277.888144	8000.365213	12.338957	-0.056294	4.815638
277.714708	8000.204280	12.343962	-0.056261	4.815592
277.545409	8000.380933	12.348967	-0.056230	4.815645
277.741135	8000.257015	12.353971	-0.056266	4.815607
277.664212	8000.201267	12.358976	-0.056251	4.815592
277.761285	8000.373734	12.363981	-0.056269	4.815641
277.821457	8000.161082	12.368986	-0.056280	4.815579
277.807752	8000.374460	12.373991	-0.056277	4.815641
277.859168	8000.418009	12.378995	-0.056287	4.815654
277.889854	8000.328773	12.384000	-0.056292	4.815628
277.744707	8000.378718	12.389005	-0.056265	4.815643
277.815044	8000.255953	12.394010	-0.056278	4.815607
277.754341	8000.281645	12.399015	-0.056267	4.815615
278.038796	8000.331143	12.404019	-0.056319	4.815628
278.121667	8000.287622	12.409024	-0.056335	4.815615
277.887245	8000.222887	12.414029	-0.056291	4.815597
277.926378	8000.310027	12.419034	-0.056298	4.815622
277.906216	8000.332110	12.424039	-0.056294	4.815629
277.946700	8000.325279	12.429043	-0.056301	4.815626
277.932703	8000.367757	12.434048	-0.056298	4.815639
277.768538	8000.477205	12.439053	-0.056268	4.815672
277.839211	8000.362990	12.444058	-0.056281	4.815638
277.708667	8000.387539	12.449063	-0.056256	4.815646
277.860379	8000.278922	12.454067	-0.056284	4.815613
277.751526	8000.326257	12.459072	-0.056264	4.815628
277.792845	8000.365368	12.464077	-0.056271	4.815639
277.935440	8000.301462	12.469082	-0.056298	4.815620
277.716539	8000.390788	12.474087	-0.056257	4.815647
277.736222	8000.406046	12.479091	-0.056260	4.815651
277.939380	8000.187189	12.484096	-0.056298	4.815586
277.852051	8000.447428	12.489101	-0.056281	4.815663
277.933514	8000.214830	12.494106	-0.056296	4.815594
277.771553	8000.300815	12.499111	-0.056266	4.815620
277.878001	8000.392261	12.504115	-0.056286	4.815646
277.911261	8000.293454	12.509120	-0.056292	4.815617
277.809939	8000.487243	12.514125	-0.056273	4.815675
277.870706	8000.358979	12.519130	-0.056284	4.815637
277.730152	8000.362003	12.524135	-0.056257	4.815638
277.875164	8000.296000	12.529139	-0.056284	4.815618
277.733854	8000.282991	12.534144	-0.056258	4.815615
277.767804	8000.406361	12.539149	-0.056264	4.815651
277.838096	8000.341272	12.544154	-0.056277	4.815632
277.685757	8000.410325	12.549159	-0.056248	4.815653
277.933236	8000.208214	12.554163	-0.056294	4.815592
277.888296	8000.131627	12.559168	-0.056285	4.815570
277.985964	8000.238950	12.564173	-0.056303	4.815601
278.030591	8000.238595	12.569178	-0.056311	4.815601
278.079151	8000.341910	12.574183	-0.056320	4.815631
277.974011	8000.369012	12.579187	-0.056301	4.815639
277.769592	8000.310109	12.584192	-0.056262	4.815623
278.004194	8000.239163	12.589197	-0.056306	4.815601
278.147287	8000.190219	12.594202	-0.056332	4.815586
277.872193	8000.286103	12.599207	-0.056281	4.815616
278.063104	8000.340478	12.604211	-0.056316	4.815631
278.030996	8000.295076	12.609216	-0.056310	4.815617
277.852287	8000.225913	12.614221	-0.056276	4.815598
277.723749	8000.238747	12.619226	-0.056252	4.815602
277.826440	8000.288474	12.624231	-0.056271	4.815616
277.855868	8000.221648	12.629235	-0.056277	4.815597
278.023086	8000.338654	12.634240	-0.056308	4.815630
277.987782	8000.308153	12.639245	-0.056301	4.815621
277.995169	8000.363798	12.644250	-0.056302	4.815638
277.849913	8000.347519	12.649255	-0.056275	4.815634
278.029154	8000.277804	12.654259	-0.056308	4.815612
278.197105	8000.364916	12.659264	-0.056339	4.815637
278.010616	8000.392822	12.664269	-0.056304	4.815646
278.053839	8000.239706	12.669274	-0.056312	4.815601
278.231591	8000.415631	12.674279	-0.056345	4.815652
278.004826	8000.259164	12.679283	-0.056302	4.815607
277.870022	8000.115953	12.684288	-0.056277	4.815566
277.907464	8000.267150	12.689293	-0.056284	4.815610
278.095784	8000.148451	12.694298	-0.056319	4.815574
277.980612	8000.526795	12.699303	-0.056297	4.815685
277.937567	8000.080676	12.704307	-0.056289	4.815555
278.118243	8000.259850	12.709312	-0.056322	4.815607
277.663098	8000.322881	12.714317	-0.056237	4.815627
277.820038	8000.299798	12.719322	-0.056266	4.815620
277.703907	8000.458096	12.724327	-0.056245	4.815667
277.858171	8000.428560	12.729331	-0.056273	4.815657
277.892674	8000.259280	12.734336	-0.056279	4.815608
277.866862	8000.398762	12.739341	-0.056274	4.815649
278.134427	8000.371080	12.744346	-0.056324	4.815639
277.836419	8000.464452	12.749351	-0.056268	4.815668
277.915595	8000.353580	12.754355	-0.056283	4.815635
278.136724	8000.179876	12.759360	-0.056324	4.815583
277.850260	8000.133518	12.764365	-0.056270	4.815571
277.898230	8000.203711	12.769370	-0.056279	4.815592
277.791424	8000.220105	12.774375	-0.056259	4.815597
277.788309	8000.274510	12.779379	-0.056258	4.815613
277.888608	8000.393625	12.784384	-0.056277	4.815647
277.785358	8000.464550	12.789389	-0.056257	4.815668
277.887883	8000.209866	12.794394	-0.056276	4.815593
277.819377	8000.316606	12.799399	-0.056263	4.815625
277.693219	8000.240827	12.804403	-0.056240	4.815603
277.675311	8000.307807	12.809408	-0.056236	4.815623
277.680235	8000.400795	12.814413	-0.056237	4.815650
277.828245	8000.376498	12.819418	-0.056264	4.815642
277.882434	8000.398729	12.824423	-0.056274	4.815649
277.899281	8000.311404	12.829427	-0.056277	4.815623
277.791180	8000.353410	12.834432	-0.056257	4.815636
277.840777	8000.422564	12.839437	-0.056266	4.815656
278.158412	8000.146833	12.844442	-0.056325	4.815574
278.037951	8000.411871	12.849447	-0.056302	4.815652
277.967213	8000.183191	12.854451	-0.056289	4.815585
278.004951	8000.197677	12.859456	-0.056295	4.815589
277.997581	8000.367367	12.864461	-0.056294	4.815639
277.971446	8000.284679	12.869466	-0.056289	4.815615
277.944721	8000.355788	12.874471	-0.056284	4.815636
278.099071	8000.279257	12.879475	-0.056312	4.815613
278.079916	8000.320582	12.884480	-0.056309	4.815625
277.989453	8000.166347	12.889485	-0.056291	4.815580
278.073873	8000.346084	12.894490	-0.056307	4.815632
277.795647	8000.386375	12.899495	-0.056255	4.815646
278.086954	8000.192458	12.904499	-0.056309	4.815587
278.092716	8000.292937	12.909504	-0.056310	4.815617
277.969766	8000.333632	12.914509	-0.056287	4.815629
278.122091	8000.281634	12.919514	-0.056315	4.815613
277.962843	8000.311055	12.924519	-0.056285	4.815623
278.026440	8000.280036	12.929523	-0.056297	4.815613
278.145654	8000.362077	12.934528	-0.056319	4.815637
277.979538	8000.399930	12.939533	-0.056288	4.815649
278.264117	8000.339416	12.944538	-0.056341	4.815630
278.178295	8000.378582	12.949543	-0.056324	4.815641
277.928308	8000.404382	12.954547	-0.056278	4.815650
278.104410	8000.385884	12.959552	-0.056310	4.815644
277.988768	8000.322025	12.964557	-0.056288	4.815626
278.100993	8000.207422	12.969562	-0.056309	4.815592
278.082146	8000.363039	12.974567	-0.056306	4.815637
278.147950	8000.195339	12.979571	-0.056317	4.815588
278.324834	8000.357364	12.984576	-0.056350	4.815635
278.105303	8000.289668	12.989581	-0.056309	4.815616
278.291292	8000.200838	12.994586	-0.056344	4.815589
278.186133	8000.300570	12.999591	-0.056324	4.815619
277.914070	8000.196769	13.004595	-0.056273	4.815590
278.163118	8000.302296	13.009600	-0.056319	4.815619
278.087386	8000.415327	13.014605	-0.056305	4.815653
277.954491	8000.161064	13.019610	-0.056280	4.815579
277.936796	8000.346607	13.024615	-0.056277	4.815633
278.038679	8000.395254	13.029619	-0.056295	4.815647
278.145597	8000.254928	13.034624	-0.056315	4.815606
277.837746	8000.398340	13.039629	-0.056258	4.815649
278.093646	8000.320267	13.044634	-0.056305	4.815625
278.163796	8000.228473	13.049639	-0.056318	4.815598
277.911774	8000.267057	13.054643	-0.056271	4.815610
278.037596	8000.130246	13.059648	-0.056294	4.815570
278.022105	8000.322233	13.064653	-0.056291	4.815626
278.035359	8000.191057	13.069658	-0.056293	4.815587
277.752761	8000.177873	13.074663	-0.056240	4.815585
277.877611	8000.363610	13.079667	-0.056263	4.815639
277.964908	8000.260348	13.084672	-0.056279	4.815608
277.875034	8000.461800	13.089677	-0.056263	4.815667
277.870190	8000.344212	13.094682	-0.056261	4.815633
277.972614	8000.327714	13.099687	-0.056280	4.815628
277.909367	8000.429200	13.104691	-0.056268	4.815658
277.922407	8000.276658	13.109696	-0.056271	4.815613
277.870622	8000.396489	13.114701	-0.056261	4.815648
277.875526	8000.128461	13.119706	-0.056261	4.815570
277.701126	8000.325324	13.124711	-0.056229	4.815628
277.750625	8000.160563	13.129715	-0.056238	4.815580
277.928830	8000.222206	13.134720	-0.056271	4.815597
277.779398	8000.246447	13.139725	-0.056243	4.815605
277.711454	8000.312608	13.144730	-0.056230	4.815625
277.815132	8000.319628	13.149735	-0.056249	4.815626
277.719399	8000.233665	13.154739	-0.056231	4.815601
277.760146	8000.383848	13.159744	-0.056238	4.815645
277.759116	8000.374202	13.164749	-0.056238	4.815642
277.805961	8000.196580	13.169754	-0.056246	4.815590
277.742916	8000.315158	13.174759	-0.056235	4.815625
277.896727	8000.310181	13.179763	-0.056263	4.815623
277.989874	8000.369365	13.184768	-0.056280	4.815640
277.686713	8000.453040	13.189773	-0.056224	4.815666
277.570753	8000.375291	13.194778	-0.056202	4.815644
277.854665	8000.392737	13.199783	-0.056255	4.815647
277.828107	8000.355970	13.204787	-0.056249	4.815637
277.801532	8000.399310	13.209792	-0.056244	4.815650
277.910914	8000.490804	13.214797	-0.056264	4.815676
277.834334	8000.232122	13.219802	-0.056250	4.815601
277.693368	8000.292816	13.224807	-0.056223	4.815619
277.732752	8000.405594	13.229811	-0.056231	4.815652
277.935521	8000.260429	13.234816	-0.056268	4.815608
277.949667	8000.375998	13.239821	-0.056271	4.815642
277.737366	8000.263562	13.244826	-0.056231	4.815610
277.803868	8000.390669	13.249831	-0.056243	4.815647
277.865328	8000.393793	13.254835	-0.056254	4.815648
277.749809	8000.287213	13.259840	-0.056233	4.815617
277.937531	8000.451551	13.264845	-0.056268	4.815664
278.029522	8000.332343	13.269850	-0.056284	4.815629
277.739544	8000.391668	13.274855	-0.056230	4.815648
277.917768	8000.582554	13.279859	-0.056263	4.815703
277.952084	8000.399384	13.284864	-0.056269	4.815649
277.967610	8000.427392	13.289869	-0.056272	4.815657
277.910293	8000.181843	13.294874	-0.056261	4.815586
277.853523	8000.333635	13.299879	-0.056250	4.815630
277.979416	8000.184008	13.304883	-0.056274	4.815586
278.209610	8000.249707	13.309888	-0.056316	4.815604
277.802814	8000.384023	13.314893	-0.056240	4.815645
278.011257	8000.384213	13.319898	-0.056279	4.815644
277.963237	8000.334277	13.324903	-0.056270	4.815630
278.000326	8000.346617	13.329907	-0.056277	4.815633
278.176166	8000.380452	13.334912	-0.056309	4.815642
278.008752	8000.392649	13.339917	-0.056278	4.815647
278.116913	8000.249140	13.344922	-0.056298	4.815604
277.964222	8000.306439	13.349927	-0.056269	4.815622
277.935734	8000.372178	13.354931	-0.056264	4.815641
277.814515	8000.247347	13.359936	-0.056241	4.815605
277.749221	8000.387250	13.364941	-0.056229	4.815646
277.865152	8000.501281	13.369946	-0.056250	4.815679
277.724040	8000.416711	13.374951	-0.056224	4.815655
277.941314	8000.348686	13.379955	-0.056264	4.815634
277.832435	8000.336207	13.384960	-0.056243	4.815631
277.853639	8000.456165	13.389965	-0.056247	4.815666
277.891312	8000.309366	13.394970	-0.056254	4.815623
278.275072	8000.325241	13.399975	-0.056325	4.815626
278.176222	8000.343901	13.404979	-0.056307	4.815632
278.148119	8000.262248	13.409984	-0.056301	4.815608
278.019507	8000.475884	13.414989	-0.056277	4.815671
278.097586	8000.259252	13.419994	-0.056291	4.815607
277.932591	8000.396456	13.424999	-0.056260	4.815648
277.800411	8000.364370	13.430003	-0.056236	4.815640
278.088724	8000.269737	13.435008	-0.056289	4.815611
277.979633	8000.415333	13.440013	-0.056269	4.815654
278.061372	8000.290618	13.445018	-0.056284	4.815617
278.066918	8000.408183	13.450023	-0.056284	4.815651
278.262943	8000.318449	13.455027	-0.056321	4.815624
278.134379	8000.263991	13.460032	-0.056297	4.815609
278.027060	8000.262218	13.465037	-0.056276	4.815609
278.040913	8000.184457	13.470042	-0.056279	4.815586
277.926440	8000.333169	13.475047	-0.056257	4.815630
277.926098	8000.246631	13.480051	-0.056257	4.815605
277.996109	8000.239214	13.485056	-0.056270	4.815602
278.053214	8000.378985	13.490061	-0.056280	4.815643
278.122757	8000.325633	13.495066	-0.056293	4.815627
278.106192	8000.278348	13.500071	-0.056290	4.815613
278.030029	8000.357193	13.505075	-0.056275	4.815636
278.109831	8000.337120	13.510080	-0.056290	4.815630
277.847535	8000.227070	13.515085	-0.056241	4.815599
277.912989	8000.354159	13.520090	-0.056253	4.815636
278.117810	8000.333995	13.525095	-0.056291	4.815629
277.953165	8000.408188	13.530099	-0.056260	4.815652
277.980273	8000.300736	13.535104	-0.056265	4.815620
278.050809	8000.293329	13.540109	-0.056278	4.815618
277.979298	8000.323117	13.545114	-0.056264	4.815627
278.049886	8000.285803	13.550119	-0.056277	4.815616
278.051543	8000.406509	13.555123	-0.056278	4.815651
278.081409	8000.311919	13.560128	-0.056283	4.815623
278.049773	8000.318862	13.565133	-0.056277	4.815625
278.225665	8000.285407	13.570138	-0.056309	4.815615
278.263500	8000.384275	13.575143	-0.056316	4.815643
278.081640	8000.347103	13.580147	-0.056282	4.815633
278.184076	8000.357307	13.585152	-0.056301	4.815636
278.131202	8000.391673	13.590157	-0.056291	4.815646
277.941180	8000.343686	13.595162	-0.056255	4.815633
277.859905	8000.378655	13.600167	-0.056240	4.815644
277.862980	8000.393642	13.605171	-0.056241	4.815648
278.071797	8000.301980	13.610176	-0.056279	4.815620
277.894638	8000.299065	13.615181	-0.056246	4.815620
278.018004	8000.219891	13.620186	-0.056269	4.815596
278.096422	8000.348261	13.625191	-0.056283	4.815634
277.894682	8000.257360	13.630195	-0.056245	4.815608
277.828017	8000.219937	13.635200	-0.056233	4.815597
277.953825	8000.296745	13.640205	-0.056256	4.815619
278.068868	8000.252682	13.645210	-0.056277	4.815606
278.222310	8000.435685	13.650215	-0.056306	4.815659
278.186348	8000.413718	13.655219	-0.056299	4.815652
278.163199	8000.159114	13.660224	-0.056294	4.815578
278.140329	8000.408658	13.665229	-0.056290	4.815651
278.202949	8000.319945	13.670234	-0.056301	4.815625
278.265150	8000.276086	13.675239	-0.056313	4.815612
277.928142	8000.501265	13.680243	-0.056250	4.815679
277.973569	8000.279826	13.685248	-0.056258	4.815614
277.879514	8000.463052	13.690253	-0.056240	4.815668
278.169829	8000.253097	13.695258	-0.056294	4.815606
278.096051	8000.369364	13.700263	-0.056280	4.815640
277.886538	8000.403302	13.705267	-0.056241	4.815651
277.983286	8000.354668	13.710272	-0.056259	4.815636
277.800880	8000.398663	13.715277	-0.056225	4.815650
278.030317	8000.328701	13.720282	-0.056267	4.815628
278.101602	8000.391801	13.725287	-0.056280	4.815646
278.061792	8000.421039	13.730291	-0.056273	4.815655
278.155036	8000.243107	13.735296	-0.056290	4.815603
278.134733	8000.388020	13.740301	-0.056286	4.815645
278.163185	8000.338267	13.745306	-0.056291	4.815631
278.046300	8000.135536	13.750311	-0.056269	4.815572
277.937542	8000.432807	13.755315	-0.056249	4.815659
278.142346	8000.192614	13.760320	-0.056286	4.815588
278.126253	8000.354685	13.765325	-0.056283	4.815636
278.113573	8000.372619	13.770330	-0.056281	4.815641
278.111412	8000.259348	13.775335	-0.056280	4.815608
277.994468	8000.372772	13.780339	-0.056258	4.815641
278.017943	8000.360322	13.785344	-0.056262	4.815638
278.061638	8000.356748	13.790349	-0.056270	4.815636
278.099861	8000.195006	13.795354	-0.056277	4.815589
277.966253	8000.324179	13.800359	-0.056252	4.815627
277.898263	8000.403157	13.805363	-0.056239	4.815651
278.239471	8000.233554	13.810368	-0.056303	4.815600
278.059585	8000.381196	13.815373	-0.056269	4.815644
278.098178	8000.218392	13.820378	-0.056276	4.815596
278.404901	8000.320590	13.825383	-0.056333	4.815624
278.173406	8000.392621	13.830387	-0.056290	4.815646
278.248701	8000.252847	13.835392	-0.056303	4.815605
278.185420	8000.378898	13.840397	-0.056292	4.815642
278.152257	8000.335615	13.845402	-0.056285	4.815630
278.093623	8000.196854	13.850407	-0.056274	4.815590
278.143180	8000.389906	13.855411	-0.056283	4.815646
278.063764	8000.282847	13.860416	-0.056268	4.815615
278.063370	8000.345842	13.865421	-0.056268	4.815633
277.909948	8000.267480	13.870426	-0.056239	4.815611
278.097913	8000.175478	13.875431	-0.056274	4.815583
278.058871	8000.239976	13.880435	-0.056266	4.815602
278.121039	8000.287973	13.885440	-0.056278	4.815616
278.228542	8000.317485	13.890445	-0.056298	4.815624
278.119558	8000.312481	13.895450	-0.056277	4.815623
278.141738	8000.288261	13.900455	-0.056281	4.815616
278.026598	8000.410260	13.905459	-0.056259	4.815652
278.183586	8000.148991	13.910464	-0.056288	4.815575
278.029888	8000.314150	13.915469	-0.056260	4.815624
278.133087	8000.263485	13.920474	-0.056279	4.815609
278.350052	8000.254201	13.925479	-0.056319	4.815605
278.170504	8000.065399	13.930483	-0.056285	4.815551
278.296252	8000.189201	13.935488	-0.056308	4.815587
278.095296	8000.346111	13.940493	-0.056271	4.815633
278.177264	8000.350640	13.945498	-0.056286	4.815634
278.225678	8000.286261	13.950503	-0.056295	4.815615
278.050357	8000.394458	13.955507	-0.056262	4.815648
278.186770	8000.352881	13.960512	-0.056287	4.815635
278.047585	8000.368744	13.965517	-0.056261	4.815640
278.028923	8000.194323	13.970522	-0.056257	4.815589
278.142339	8000.196161	13.975527	-0.056278	4.815589
278.122889	8000.329338	13.980531	-0.056274	4.815628
278.048032	8000.244785	13.985536	-0.056260	4.815604
278.253194	8000.419021	13.990541	-0.056298	4.815654
278.356747	8000.192124	13.995546	-0.056317	4.815587
278.323387	8000.295167	14.000551	-0.056311	4.815617
278.248002	8000.264010	14.005555	-0.056297	4.815609
278.394055	8000.147824	14.010560	-0.056324	4.815574
278.261656	8000.395577	14.015565	-0.056299	4.815647
278.228579	8000.365112	14.020570	-0.056293	4.815638
278.325555	8000.378431	14.025575	-0.056311	4.815642
278.312376	8000.336542	14.030579	-0.056308	4.815630
278.177881	8000.374912	14.035584	-0.056283	4.815641
278.065600	8000.383739	14.040589	-0.056262	4.815645
278.235593	8000.381164	14.045594	-0.056293	4.815643
278.288431	8000.317925	14.050599	-0.056303	4.815624
278.049223	8000.340697	14.055603	-0.056258	4.815632
278.060264	8000.145399	14.060608	-0.056260	4.815575
278.027975	8000.481305	14.065613	-0.056254	4.815673
278.086344	8000.357275	14.070618	-0.056264	4.815637
278.218528	8000.423507	14.075623	-0.056289	4.815656
278.199463	8000.401816	14.080627	-0.056285	4.815649
278.125485	8000.268144	14.085632	-0.056271	4.815611
278.119556	8000.407952	14.090637	-0.056270	4.815651
278.119558	8000.387641	14.095642	-0.056269	4.815646
278.016787	8000.381670	14.100647	-0.056250	4.815644
278.002033	8000.385684	14.105651	-0.056247	4.815646
278.208511	8000.348458	14.110656	-0.056285	4.815634
278.095703	8000.395728	14.115661	-0.056264	4.815648
278.047080	8000.375690	14.120666	-0.056255	4.815642
277.950049	8000.279025	14.125671	-0.056237	4.815615
278.023602	8000.442562	14.130675	-0.056250	4.815662
278.198497	8000.304417	14.135680	-0.056283	4.815621
278.053347	8000.385337	14.140685	-0.056255	4.815645
278.132333	8000.373796	14.145690	-0.056270	4.815641
278.255404	8000.289276	14.150695	-0.056293	4.815616
278.180885	8000.452528	14.155699	-0.056279	4.815664
278.183738	8000.268844	14.160704	-0.056279	4.815611
278.264734	8000.266948	14.165709	-0.056294	4.815610
278.195098	8000.292495	14.170714	-0.056281	4.815617
278.250380	8000.384171	14.175719	-0.056291	4.815644
278.206674	8000.366349	14.180723	-0.056282	4.815639
278.252779	8000.168420	14.185728	-0.056291	4.815581
278.066522	8000.376839	14.190733	-0.056256	4.815643
278.056326	8000.246348	14.195738	-0.056254	4.815605
278.151438	8000.275658	14.200743	-0.056271	4.815613
277.874735	8000.412102	14.205747	-0.056220	4.815654
277.997896	8000.212231	14.210752	-0.056242	4.815595
278.157101	8000.410280	14.215757	-0.056272	4.815652
278.102554	8000.465980	14.220762	-0.056262	4.815669
278.083159	8000.328929	14.225767	-0.056258	4.815629
278.059278	8000.268708	14.230771	-0.056253	4.815611
278.220241	8000.286278	14.235776	-0.056283	4.815616
278.186767	8000.249398	14.240781	-0.056276	4.815605
278.119635	8000.367910	14.245786	-0.056264	4.815640
278.023809	8000.278741	14.250791	-0.056246	4.815614
277.998278	8000.397933	14.255795	-0.056241	4.815649
277.917867	7999.444953	14.260800	-0.056225	4.815371
277.960298	7996.269591	14.265805	-0.056231	4.814443
278.045758	7990.733046	14.270810	-0.056243	4.812823
277.984208	7983.972063	14.275815	-0.056227	4.810846
277.982982	7976.615426	14.280819	-0.056221	4.808693
278.016445	7969.040891	14.285824	-0.056223	4.806475
277.957964	7961.208435	14.290829	-0.056206	4.804181
277.971590	7953.351027	14.295834	-0.056204	4.801878
278.028258	7945.434168	14.300839	-0.056209	4.799557
277.806242	7937.430808	14.305843	-0.056162	4.797210
277.731836	7929.395334	14.310848	-0.056143	4.794852
278.042085	7921.371534	14.315853	-0.056195	4.792494
277.804193	7913.323573	14.320858	-0.056145	4.790131
277.813712	7905.396787	14.325863	-0.056142	4.787801
277.716211	7897.335462	14.330867	-0.056118	4.785431
277.733200	7889.430383	14.335872	-0.056116	4.783105
277.591365	7881.423099	14.340877	-0.056084	4.780748
277.568919	7873.415053	14.345882	-0.056075	4.778390
277.710948	7865.429021	14.350887	-0.056096	4.776036
277.405970	7857.386059	14.355891	-0.056033	4.773666
277.302928	7849.358248	14.360896	-0.056009	4.771299
277.579315	7841.398449	14.365901	-0.056055	4.768949
277.376665	7833.363630	14.370906	-0.056012	4.766578
277.358634	7825.366835	14.375911	-0.056003	4.764216
277.328163	7817.383378	14.380915	-0.055992	4.761856
277.402006	7809.372399	14.385920	-0.056000	4.759487
277.355518	7801.422030	14.390925	-0.055986	4.757135
277.569018	7793.360461	14.395930	-0.056021	4.754749
277.538481	7785.328603	14.400935	-0.056009	4.752370
277.393162	7777.276351	14.405939	-0.055977	4.749985
277.302129	7769.313030	14.410944	-0.055955	4.747625
277.392101	7761.319844	14.415949	-0.055966	4.745254
277.242511	7753.357594	14.420954	-0.055933	4.742892
277.147953	7745.368395	14.425959	-0.055910	4.740520
277.108314	7737.332298	14.430963	-0.055897	4.738134
277.058829	7729.347441	14.435968	-0.055882	4.735761
277.020774	7721.367774	14.440973	-0.055870	4.733389
276.822196	7713.269956	14.445978	-0.055827	4.730980
277.040873	7705.331208	14.450983	-0.055863	4.728617
276.807024	7697.250765	14.455987	-0.055814	4.726211
276.823965	7689.351707	14.460992	-0.055812	4.723858
276.886476	7681.344939	14.465997	-0.055818	4.721471
276.855686	7673.280714	14.471002	-0.055807	4.719066
276.972441	7665.322260	14.476007	-0.055823	4.716691
276.889032	7657.306570	14.481011	-0.055802	4.714299
277.048276	7649.327205	14.486016	-0.055826	4.711915
276.937732	7641.287087	14.491021	-0.055800	4.709513
276.652444	7633.307233	14.496026	-0.055742	4.707128
276.851468	7625.279769	14.501031	-0.055773	4.704726
276.595922	7617.335501	14.506035	-0.055720	4.702349
276.606362	7609.287746	14.511040	-0.055717	4.699939
276.456506	7601.311807	14.516045	-0.055684	4.697550
276.569688	7593.274023	14.521050	-0.055699	4.695140
276.590773	7585.343823	14.526055	-0.055698	4.692762
276.245109	7577.263529	14.531059	-0.055628	4.690338
276.549509	7569.301611	14.536064	-0.055679	4.687947
276.354430	7561.267005	14.541069	-0.055638	4.685534
276.304931	7553.293512	14.546074	-0.055623	4.683138
276.362333	7545.309128	14.551079	-0.055628	4.680737
276.231301	7537.314370	14.556083	-0.055598	4.678332
276.270344	7529.313218	14.561088	-0.055600	4.675924
276.275420	7521.211339	14.566093	-0.055596	4.673484
276.265482	7513.147815	14.571098	-0.055588	4.671054
276.161451	7505.215436	14.576103	-0.055564	4.668663
276.090375	7497.194174	14.581107	-0.055545	4.666244
276.003145	7489.237032	14.586112	-0.055523	4.663843
276.184542	7481.305725	14.591117	-0.055552	4.661448
276.112490	7473.203939	14.596122	-0.055533	4.659001
276.223867	7465.247516	14.601127	-0.055548	4.656596
276.042706	7457.166243	14.606131	-0.055509	4.654152
276.065866	7449.227113	14.611136	-0.055508	4.651750
275.779538	7441.185009	14.616141	-0.055449	4.649316
275.719583	7433.227182	14.621146	-0.055433	4.646906
275.823578	7425.254347	14.626151	-0.055447	4.644490
275.590878	7417.249871	14.631155	-0.055398	4.642063
275.656655	7409.208108	14.636160	-0.055405	4.639623
275.657918	7401.230083	14.641165	-0.055400	4.637202
275.640815	7393.169866	14.646170	-0.055391	4.634754
275.772716	7385.188106	14.651175	-0.055410	4.632329
275.744500	7377.174343	14.656179	-0.055400	4.629893
275.596265	7369.177001	14.661184	-0.055367	4.627461
275.590028	7361.163545	14.666189	-0.055360	4.625022
275.614333	7353.218929	14.671194	-0.055359	4.622603
275.717928	7345.188349	14.676199	-0.055373	4.620157
275.369900	7337.206908	14.681203	-0.055303	4.617724
275.656761	7329.143918	14.686208	-0.055351	4.615265
275.602937	7321.148571	14.691213	-0.055335	4.612826
275.381474	7313.137082	14.696218	-0.055289	4.610380
275.532506	7305.191076	14.701223	-0.055311	4.607953
275.458842	7297.138032	14.706227	-0.055292	4.605492
275.387107	7289.185280	14.711232	-0.055274	4.603060
275.456120	7281.146840	14.716237	-0.055281	4.600601
275.410079	7273.158709	14.721242	-0.055267	4.598156
275.502873	7265.174655	14.726247	-0.055279	4.595710
275.149656	7257.119154	14.731251	-0.055208	4.593242
275.110439	7249.074685	14.736256	-0.055195	4.590775
275.169021	7241.157481	14.741261	-0.055201	4.588347
275.023434	7233.054739	14.746266	-0.055168	4.585860
275.110276	7225.184586	14.751271	-0.055179	4.583443
274.951773	7217.096725	14.756275	-0.055144	4.580958
275.037552	7209.148691	14.761280	-0.055154	4.578515
274.978646	7201.123112	14.766285	-0.055138	4.576046
274.751887	7193.127784	14.771290	-0.055090	4.573585
275.016423	7185.095667	14.776295	-0.055134	4.571112
275.035490	7177.128451	14.781299	-0.055132	4.568658
274.928864	7169.099161	14.786304	-0.055107	4.566183
275.005297	7161.119093	14.791309	-0.055116	4.563722
274.690695	7153.123688	14.796314	-0.055052	4.561254
274.600444	7145.169171	14.801319	-0.055030	4.558798
274.941964	7137.148324	14.806323	-0.055088	4.556321
274.899215	7129.117374	14.811328	-0.055075	4.553838
274.745598	7121.093392	14.816333	-0.055041	4.551357
274.778650	7113.074918	14.821338	-0.055041	4.548876
274.818481	7105.118244	14.826343	-0.055043	4.546412
274.608818	7097.088654	14.831347	-0.054999	4.543925
274.520307	7089.138390	14.836352	-0.054977	4.541461
274.607976	7081.106903	14.841357	-0.054988	4.538970
274.426858	7073.147823	14.846362	-0.054949	4.536500
274.384757	7065.096774	14.851367	-0.054936	4.534001
274.261292	7057.102968	14.856371	-0.054907	4.531518
274.278083	7049.067473	14.861376	-0.054905	4.529020
274.264336	7041.088815	14.866381	-0.054897	4.526539
274.339456	7033.094859	14.871386	-0.054905	4.524052
274.399638	7025.154515	14.876391	-0.054911	4.521581
274.207552	7017.103131	14.881395	-0.054870	4.519072
274.174149	7009.164256	14.886400	-0.054859	4.516598
274.232849	7001.070881	14.891405	-0.054864	4.514075
274.207470	6993.017705	14.896410	-0.054854	4.511562
274.073870	6985.037912	14.901415	-0.054824	4.509071
274.258968	6977.021938	14.906419	-0.054853	4.506568
274.202946	6969.048382	14.911424	-0.054837	4.504076
274.121459	6961.097460	14.916429	-0.054816	4.501589
273.821236	6953.073128	14.921434	-0.054755	4.499078
273.888106	6945.100883	14.926439	-0.054762	4.496582
273.850690	6937.043342	14.931443	-0.054750	4.494059
273.688893	6929.058269	14.936448	-0.054714	4.491556
273.865337	6921.037588	14.941453	-0.054741	4.489041
273.648984	6913.048132	14.946458	-0.054696	4.486534
273.752074	6905.086838	14.951463	-0.054710	4.484035
273.642144	6897.058620	14.956467	-0.054684	4.481513
273.797225	6889.085810	14.961472	-0.054707	4.479008
273.793685	6881.080400	14.966477	-0.054701	4.476491
273.735625	6873.060257	14.971482	-0.054685	4.473967
273.805140	6865.028381	14.976487	-0.054692	4.471439
273.740651	6857.026326	14.981491	-0.054675	4.468918
273.667176	6849.023972	14.986496	-0.054656	4.466396
273.479311	6841.054238	14.991501	-0.054616	4.463882
273.599206	6833.022106	14.996506	-0.054632	4.461348
273.609650	6825.085789	15.001511	-0.054629	4.458843
273.456482	6817.030458	15.006515	-0.054595	4.456298
273.316191	6809.038889	15.011520	-0.054564	4.453772
273.288033	6800.963646	15.016525	-0.054553	4.451218
273.209255	6792.979524	15.021530	-0.054533	4.448691
273.208877	6785.013741	15.026535	-0.054527	4.446169
272.999692	6777.019783	15.031539	-0.054483	4.443636
272.977185	6769.014180	15.036544	-0.054473	4.441099
273.006283	6761.040022	15.041549	-0.054473	4.438570
273.209518	6753.007016	15.046554	-0.054506	4.436022
273.110084	6744.996560	15.051559	-0.054482	4.433478
273.036383	6736.954034	15.056563	-0.054463	4.430922
273.133979	6728.998158	15.061568	-0.054476	4.428394
273.029885	6720.956516	15.066573	-0.054451	4.425836
272.740931	6712.998807	15.071578	-0.054392	4.423302
272.912246	6704.976149	15.076583	-0.054418	4.420748
272.916797	6697.001744	15.081587	-0.054413	4.418207
272.767985	6688.974569	15.086592	-0.054380	4.415648
272.859418	6681.012955	15.091597	-0.054392	4.413109
272.744160	6672.934959	15.096602	-0.054365	4.410530
272.911986	6664.973527	15.101607	-0.054391	4.407988
272.510830	6656.946702	15.106611	-0.054311	4.405421
272.596149	6649.010485	15.111616	-0.054321	4.402884
272.609050	6641.015623	15.116621	-0.054318	4.400327
272.355139	6633.008425	15.121626	-0.054266	4.397762
272.500938	6625.008012	15.126631	-0.054287	4.395201
272.501526	6616.953344	15.131635	-0.054282	4.392619
272.357781	6608.938037	15.136640	-0.054250	4.390048
272.488608	6601.016071	15.141645	-0.054269	4.387507
272.579897	6592.923381	15.146650	-0.054280	4.384910
272.474967	6585.015806	15.151655	-0.054256	4.382369
272.251059	6576.947025	15.156659	-0.054208	4.379775
272.521135	6569.023548	15.161664	-0.054253	4.377228
272.521082	6560.995122	15.166669	-0.054248	4.374644
272.071336	6552.958518	15.171674	-0.054159	4.372054
272.146240	6544.958624	15.176679	-0.054167	4.369477
272.119733	6536.973107	15.181683	-0.054157	4.366903
272.109852	6528.975548	15.186688	-0.054150	4.364323
271.874856	6521.043195	15.191693	-0.054101	4.361762
271.915285	6512.960393	15.196698	-0.054103	4.359152
272.288201	6505.048726	15.201703	-0.054167	4.356597
272.024069	6496.930359	15.206707	-0.054112	4.353971
272.061446	6488.881335	15.211712	-0.054114	4.351367
271.919902	6480.925621	15.216717	-0.054082	4.348791
271.766921	6472.914215	15.221722	-0.054048	4.346195
271.780391	6464.959095	15.226727	-0.054045	4.343617
271.734114	6456.948360	15.231731	-0.054031	4.341019
271.754819	6448.992006	15.236736	-0.054030	4.338437
271.561065	6440.968071	15.241741	-0.053988	4.335831
271.594970	6432.923001	15.246746	-0.053989	4.333217
271.583016	6424.971147	15.251751	-0.053981	4.330632
271.652820	6416.946456	15.256755	-0.053989	4.328022
271.639891	6408.914034	15.261760	-0.053981	4.325408
271.734452	6400.986626	15.266765	-0.053993	4.322827
271.478476	6392.948267	15.271770	-0.053940	4.320206
271.309810	6385.009592	15.276775	-0.053903	4.317616
271.267521	6376.944670	15.281779	-0.053890	4.314985
271.382566	6368.913559	15.286784	-0.053906	4.312364
271.283441	6360.926685	15.291789	-0.053882	4.309754
271.398355	6352.888100	15.296794	-0.053898	4.307127
271.575005	6344.928308	15.301799	-0.053926	4.304526
271.339994	6336.985010	15.306803	-0.053877	4.301924
271.190943	6328.951140	15.311808	-0.053843	4.299292
271.291850	6320.932382	15.316813	-0.053857	4.296666
271.038610	6312.920499	15.321818	-0.053804	4.294037
271.119516	6304.890167	15.326823	-0.053814	4.291403
271.085600	6296.917988	15.331827	-0.053802	4.288786
271.110618	6288.904560	15.336832	-0.053801	4.286154
271.030059	6280.920560	15.341837	-0.053781	4.283530
270.890347	6272.935406	15.346842	-0.053750	4.280903
271.048290	6264.968454	15.351847	-0.053774	4.278282
270.760595	6256.935374	15.356851	-0.053715	4.275635
270.713268	6248.857562	15.361856	-0.053700	4.272973
270.807199	6240.863470	15.366861	-0.053712	4.270338
270.713378	6232.865996	15.371866	-0.053690	4.267699
270.598133	6224.866521	15.376871	-0.053663	4.265058
270.726209	6216.914671	15.381875	-0.053681	4.262433
270.591469	6208.834064	15.386880	-0.053651	4.259761
270.717007	6200.948758	15.391885	-0.053669	4.257154
270.700276	6192.872180	15.396890	-0.053660	4.254481
270.869894	6184.922804	15.401895	-0.053686	4.251851
270.592111	6176.879553	15.406899	-0.053629	4.249183
270.388057	6168.939202	15.411904	-0.053586	4.246549
270.528431	6160.901971	15.416909	-0.053607	4.243884
270.373623	6152.926059	15.421914	-0.053572	4.241235
270.408581	6144.969517	15.426919	-0.053573	4.238593
270.385008	6136.976417	15.431923	-0.053564	4.235936
270.350529	6128.910772	15.436928	-0.053552	4.233253
270.301932	6120.874121	15.441933	-0.053537	4.230578
270.135720	6112.900390	15.446938	-0.053501	4.227921
270.282420	6104.919703	15.451943	-0.053523	4.225264
270.409389	6096.924913	15.456947	-0.053541	4.222599
270.191285	6088.926734	15.461952	-0.053495	4.219929
270.120459	6080.976027	15.466957	-0.053477	4.217274
269.988688	6072.915422	15.471962	-0.053447	4.214580
270.078796	6064.927966	15.476967	-0.053458	4.211911
270.209895	6056.898564	15.481971	-0.053477	4.209226
270.091551	6048.968663	15.486976	-0.053450	4.206571
270.062888	6040.947847	15.491981	-0.053439	4.203885
269.979771	6032.945987	15.496986	-0.053418	4.201202
270.012289	6024.953089	15.501991	-0.053419	4.198522
270.039351	6016.946859	15.506995	-0.053418	4.195836
269.869553	6008.852561	15.512000	-0.053381	4.193117
269.903859	6000.805359	15.517005	-0.053382	4.190413
270.001340	5992.874564	15.522010	-0.053395	4.187748
269.865603	5984.876561	15.527015	-0.053364	4.185056
269.688845	5976.929607	15.532019	-0.053326	4.182379
269.812283	5968.873276	15.537024	-0.053343	4.179666
269.700133	5960.925277	15.542029	-0.053317	4.176986
269.906403	5952.885810	15.547034	-0.053350	4.174277
269.962025	5944.871310	15.552039	-0.053355	4.171573
269.730097	5936.870722	15.557043	-0.053306	4.168868
269.606391	5928.923493	15.562048	-0.053278	4.166181
269.597829	5920.930469	15.567053	-0.053271	4.163478
269.578026	5912.878469	15.572058	-0.053262	4.160753
269.510295	5904.964291	15.577063	-0.053244	4.158072
269.540291	5896.890679	15.582067	-0.053244	4.155337
269.460589	5888.863930	15.587072	-0.053224	4.152615
269.365664	5880.897292	15.592077	-0.053201	4.149911
269.202404	5872.881296	15.597082	-0.053165	4.147188
269.218342	5864.894629	15.602087	-0.053163	4.144475
269.294886	5856.912878	15.607091	-0.053171	4.141762
269.046427	5848.912153	15.612096	-0.053120	4.139038
269.253918	5840.913275	15.617101	-0.053153	4.136317
269.112442	5832.870785	15.622106	-0.053121	4.133576
269.119024	5824.885096	15.627111	-0.053117	4.130854
269.000656	5816.879951	15.632115	-0.053090	4.128123
269.017359	5808.854176	15.637120	-0.053087	4.125384
268.930000	5800.911590	15.642125	-0.053066	4.122670
268.895186	5792.881919	15.647130	-0.053054	4.119926
269.040808	5784.939424	15.652135	-0.053075	4.117211
269.038227	5776.877244	15.657139	-0.053070	4.114452
268.784192	5768.852731	15.662144	-0.053017	4.111701
268.821996	5760.876398	15.667149	-0.053018	4.108969
268.742002	5752.857961	15.672154	-0.052998	4.106218
268.850730	5744.917769	15.677159	-0.053013	4.103495
268.704906	5736.889873	15.682163	-0.052980	4.100737
268.711608	5728.922419	15.687168	-0.052976	4.097999
268.901495	5720.900536	15.692173	-0.053006	4.095244
268.614269	5712.898050	15.697178	-0.052947	4.092487
268.627230	5704.893853	15.702183	-0.052944	4.089731
268.449672	5696.890778	15.707187	-0.052906	4.086972
268.629814	5688.876319	15.712192	-0.052934	4.084211
268.438764	5680.948015	15.717197	-0.052893	4.081474
268.259655	5672.924287	15.722202	-0.052854	4.078701
268.372901	5664.950372	15.727207	-0.052870	4.075948
268.177192	5656.931071	15.732211	-0.052828	4.073174
268.378589	5648.876864	15.737216	-0.052860	4.070390
268.419941	5640.957230	15.742221	-0.052863	4.067650
268.236411	5632.908869	15.747226	-0.052823	4.064859
268.496686	5624.986528	15.752231	-0.052866	4.062117
268.259671	5616.919924	15.757235	-0.052816	4.059315
268.142510	5608.943935	15.762240	-0.052789	4.056545
268.072835	5600.926544	15.767245	-0.052771	4.053759
268.031339	5592.904541	15.772250	-0.052758	4.050971
267.839110	5584.946475	15.777255	-0.052717	4.048200
267.856250	5576.923221	15.782259	-0.052714	4.045407
267.918849	5568.951068	15.787264	-0.052721	4.042632
267.892533	5560.933544	15.792269	-0.052710	4.039837
267.832072	5552.948106	15.797274	-0.052694	4.037051
267.831872	5544.931639	15.802279	-0.052688	4.034253
267.904789	5536.855922	15.807283	-0.052696	4.031433
267.797164	5528.865112	15.812288	-0.052671	4.028639
267.795386	5520.872602	15.817293	-0.052665	4.025843
267.944773	5512.917370	15.822298	-0.052688	4.023061
267.767839	5504.900864	15.827303	-0.052649	4.020251
267.713899	5496.923787	15.832307	-0.052634	4.017454
267.689143	5488.886930	15.837312	-0.052624	4.014635
267.668989	5480.927557	15.842317	-0.052615	4.011841
267.428096	5472.876115	15.847322	-0.052564	4.009010
267.419365	5464.901716	15.852327	-0.052557	4.006207
267.511068	5456.930146	15.857331	-0.052569	4.003404
267.313665	5448.916063	15.862336	-0.052527	4.000580
267.398985	5440.926744	15.867341	-0.052537	3.997768
267.353555	5432.913584	15.872346	-0.052523	3.994943
267.383844	5424.891137	15.877351	-0.052524	3.992114
267.220140	5416.874484	15.882355	-0.052488	3.989281
267.321868	5408.883106	15.887360	-0.052501	3.986460
267.482347	5400.932582	15.892365	-0.052526	3.983653
267.272769	5392.908725	15.897370	-0.052481	3.980811
267.343352	5384.953371	15.902375	-0.052489	3.977996
267.091753	5376.936868	15.907379	-0.052437	3.975152
267.002845	5368.905312	15.912384	-0.052415	3.972304
267.044274	5360.911201	15.917389	-0.052417	3.969469
267.108116	5352.920842	15.922394	-0.052424	3.966633
267.042572	5344.973123	15.927399	-0.052406	3.963809
266.959552	5336.981026	15.932403	-0.052385	3.960966
266.834382	5328.973058	15.937408	-0.052357	3.958115
266.964565	5320.950652	15.942413	-0.052375	3.955261
266.771406	5312.913809	15.947418	-0.052334	3.952395
266.757363	5304.930157	15.952423	-0.052326	3.949548
266.842946	5296.963133	15.957427	-0.052336	3.946707
266.867253	5288.935780	15.962432	-0.052336	3.943842
266.664872	5280.966520	15.967437	-0.052293	3.940990
266.694208	5272.976780	15.972442	-0.052293	3.938134
266.768732	5264.995814	15.977447	-0.052301	3.935280
266.587594	5256.960192	15.982451	-0.052262	3.932399
266.558139	5248.941215	15.987456	-0.052251	3.929525
266.636777	5240.997519	15.992461	-0.052260	3.926678
266.410316	5232.999340	15.997466	-0.052213	3.923803
266.474686	5225.037539	16.002471	-0.052219	3.920945
266.464209	5217.030633	16.007475	-0.052212	3.918067
266.371974	5208.953977	16.012480	-0.052189	3.915161
266.385410	5200.986320	16.017485	-0.052186	3.912293
266.233118	5192.957674	16.022490	-0.052153	3.909398
266.384270	5184.977346	16.027495	-0.052175	3.906525
266.403938	5176.980251	16.032499	-0.052174	3.903640
266.022042	5169.004820	16.037504	-0.052097	3.900754
266.167203	5161.029470	16.042509	-0.052119	3.897875
266.321873	5152.942058	16.047514	-0.052142	3.894954
266.218468	5144.965697	16.052519	-0.052118	3.892067
266.258231	5136.961009	16.057523	-0.052120	3.889169
266.212476	5128.988353	16.062528	-0.052106	3.886279
266.068130	5121.017442	16.067533	-0.052073	3.883386
265.999368	5112.993455	16.072538	-0.052055	3.880473
266.028852	5105.036425	16.077543	-0.052055	3.877584
265.874809	5097.029090	16.082547	-0.052021	3.874671
265.708881	5088.757348	16.087552	-0.051985	3.871659
265.825219	5080.858338	16.092557	-0.052001	3.868786
265.794859	5072.880614	16.097562	-0.051990	3.865879
265.661756	5064.968461	16.102567	-0.051960	3.862993
265.622485	5056.962182	16.107571	-0.051947	3.860071
265.520043	5048.979999	16.112576	-0.051923	3.857155
265.590394	5040.993502	16.117581	-0.051930	3.854238
265.646421	5032.945541	16.122586	-0.051935	3.851297
265.607526	5025.003660	16.127591	-0.051923	3.848390
265.667696	5017.014549	16.132595	-0.051928	3.845465
265.369634	5009.016651	16.137600	-0.051868	3.842528
265.558830	5001.035052	16.142605	-0.051897	3.839605
265.465018	4993.049914	16.147610	-0.051875	3.836672
265.415131	4985.030211	16.152615	-0.051860	3.833725
265.567091	4976.998447	16.157619	-0.051883	3.830776
265.525672	4969.022004	16.162624	-0.051870	3.827840
265.448183	4961.066481	16.167629	-0.051850	3.824910
265.168150	4953.082132	16.172634	-0.051792	3.821962
265.305109	4945.077526	16.177639	-0.051812	3.819013
265.084215	4937.090418	16.182643	-0.051766	3.816061
264.970758	4929.059425	16.187648	-0.051739	3.813093
265.088967	4921.052513	16.192653	-0.051756	3.810136
265.030203	4913.076440	16.197658	-0.051740	3.807184
265.024709	4905.097566	16.202663	-0.051733	3.804231
264.948687	4897.104609	16.207667	-0.051714	3.801268
265.007715	4889.104917	16.212672	-0.051719	3.798303
264.906444	4881.109994	16.217677	-0.051695	3.795334
264.733822	4873.059216	16.222682	-0.051657	3.792341
264.898892	4865.054406	16.227687	-0.051683	3.789370
264.976599	4857.084519	16.232691	-0.051692	3.786407
264.711186	4849.085216	16.237696	-0.051637	3.783424
264.813805	4841.101231	16.242701	-0.051651	3.780452
264.679004	4833.097616	16.247706	-0.051620	3.777465
264.509832	4825.079054	16.252711	-0.051583	3.774470
264.511938	4817.069921	16.257715	-0.051578	3.771479
264.650692	4809.053819	16.262720	-0.051599	3.768487
264.473774	4801.115039	16.267725	-0.051560	3.765514
264.391311	4793.098452	16.272730	-0.051540	3.762511
264.505995	4785.102855	16.277735	-0.051555	3.759519
264.469394	4777.157035	16.282739	-0.051543	3.756539
264.238540	4769.111437	16.287744	-0.051495	3.753515
264.288801	4761.094059	16.292749	-0.051499	3.750506
264.291893	4753.095170	16.297754	-0.051494	3.747500
264.291549	4745.097110	16.302759	-0.051489	3.744492
264.289553	4737.152018	16.307763	-0.051483	3.741501
264.295342	4729.093501	16.312768	-0.051478	3.738466
264.352932	4721.130153	16.317773	-0.051484	3.735465
264.144597	4713.132916	16.322778	-0.051440	3.732443
264.249285	4705.089361	16.327783	-0.051454	3.729408
264.244570	4697.127806	16.332787	-0.051447	3.726399
263.932118	4689.146932	16.337792	-0.051384	3.723373
264.039432	4681.183768	16.342797	-0.051398	3.720361
264.028440	4673.196708	16.347802	-0.051391	3.717335
263.881135	4665.195303	16.352807	-0.051358	3.714297
263.831242	4657.087318	16.357811	-0.051343	3.711219
263.725917	4649.090747	16.362816	-0.051318	3.708180
263.927585	4641.123549	16.367821	-0.051350	3.705156
263.871276	4633.164803	16.372826	-0.051335	3.702127
263.833601	4625.166302	16.377831	-0.051322	3.699081
263.792724	4617.222125	16.382835	-0.051309	3.696053
263.599766	4609.217548	16.387840	-0.051268	3.692996
263.535958	4601.193196	16.392845	-0.051251	3.689932
263.747852	4593.208796	16.397850	-0.051285	3.686887
263.676908	4585.216995	16.402855	-0.051266	3.683830
263.607028	4577.250555	16.407859	-0.051248	3.680780
263.446047	4569.256896	16.412864	-0.051212	3.677715
263.320740	4561.235838	16.417869	-0.051184	3.674637
263.253453	4553.209535	16.422874	-0.051166	3.671557
263.302769	4545.200049	16.427879	-0.051169	3.668483
263.139703	4537.233510	16.432883	-0.051134	3.665418
263.086451	4529.246812	16.437888	-0.051118	3.662345
263.150633	4521.249152	16.442893	-0.051125	3.659269
263.241289	4513.254775	16.447898	-0.051136	3.656192
263.134323	4505.255479	16.452903	-0.051111	3.653105
263.017785	4497.228875	16.457907	-0.051084	3.650005
262.999605	4489.244423	16.462912	-0.051075	3.646921
263.274424	4481.268387	16.467917	-0.051121	3.643846
263.167582	4473.255915	16.472922	-0.051096	3.640743
263.002131	4465.297101	16.477927	-0.051059	3.637658
262.934891	4457.294819	16.482931	-0.051041	3.634555
262.830077	4449.256959	16.487936	-0.051016	3.631435
262.808443	4441.256437	16.492941	-0.051007	3.628329
262.772986	4433.238044	16.497946	-0.050995	3.625213
262.791555	4425.278157	16.502951	-0.050993	3.622118
262.720886	4417.320119	16.507955	-0.050975	3.619019
262.663119	4409.306333	16.512960	-0.050958	3.615896
262.793909	4401.312585	16.517965	-0.050977	3.612784
262.777260	4393.264944	16.522970	-0.050969	3.609643
262.519029	4385.331800	16.527975	-0.050915	3.606538
262.521787	4377.338297	16.532979	-0.050910	3.603414
262.575889	4369.331308	16.537984	-0.050915	3.600283
262.638828	4361.396788	16.542989	-0.050922	3.597178
262.615391	4353.357444	16.547994	-0.050912	3.594027
262.725063	4345.326713	16.552999	-0.050927	3.590881
262.542261	4337.377375	16.558003	-0.050887	3.587755
262.406127	4329.350657	16.563008	-0.050857	3.584597
262.380380	4321.432571	16.568013	-0.050846	3.581483
262.368895	4313.399043	16.573018	-0.050839	3.578321
262.450900	4305.384020	16.578023	-0.050849	3.575165
262.346581	4297.399182	16.583027	-0.050824	3.572014
262.309073	4289.353279	16.588032	-0.050811	3.568838
261.970595	4281.435474	16.593037	-0.050743	3.565700
261.825578	4273.461577	16.598042	-0.050711	3.562544
261.927522	4265.430802	16.603047	-0.050724	3.559369
261.884885	4257.488006	16.608051	-0.050711	3.556222
261.958731	4249.356238	16.613056	-0.050719	3.553001
262.028698	4241.322556	16.618061	-0.050727	3.549815
261.894070	4233.382083	16.623066	-0.050696	3.546658
261.720373	4225.406139	16.628071	-0.050659	3.543483
261.800515	4217.414428	16.633075	-0.050668	3.540306
261.904991	4209.401380	16.638080	-0.050682	3.537118
261.769791	4201.451989	16.643085	-0.050652	3.533946
261.654320	4193.405046	16.648090	-0.050625	3.530732
261.820074	4185.429324	16.653095	-0.050650	3.527553
261.554758	4177.454497	16.658099	-0.050595	3.524358
261.514401	4169.473759	16.663104	-0.050582	3.521164
261.718335	4161.480815	16.668109	-0.050615	3.517971
261.539063	4153.480827	16.673114	-0.050576	3.514759
261.337319	4145.486855	16.678119	-0.050533	3.511547
261.608462	4137.483271	16.683123	-0.050578	3.508342
261.736093	4129.463804	16.688128	-0.050597	3.505124
261.403046	4121.536225	16.693133	-0.050529	3.501925
261.299578	4113.533101	16.698138	-0.050505	3.498700
261.467603	4105.522463	16.703143	-0.050531	3.495477
261.393025	4097.543496	16.708147	-0.050511	3.492257
261.167624	4089.534257	16.713152	-0.050464	3.489017
261.323813	4081.574458	16.718157	-0.050488	3.485805
261.514264	4073.563678	16.723162	-0.050518	3.482572
261.184739	4065.602791	16.728167	-0.050451	3.479338
261.145194	4057.637327	16.733171	-0.050438	3.476110
261.258855	4049.552504	16.738176	-0.050454	3.472834
261.113916	4041.571131	16.743181	-0.050421	3.469590
260.965705	4033.566838	16.748186	-0.050388	3.466332
260.882023	4025.621771	16.753191	-0.050367	3.463098
260.976761	4017.613939	16.758195	-0.050380	3.459841
260.715211	4009.648306	16.763200	-0.050326	3.456587
260.905123	4001.619582	16.768205	-0.050356	3.453319
260.860907	3993.573673	16.773210	-0.050342	3.450032
260.621787	3985.644362	16.778215	-0.050292	3.446784
260.658857	3977.630855	16.783219	-0.050294	3.443508
260.567719	3969.637655	16.788224	-0.050271	3.440232
260.559700	3961.691803	16.793229	-0.050264	3.436976
260.588104	3953.653908	16.798234	-0.050264	3.433679
260.565793	3945.607349	16.803239	-0.050255	3.430375
260.616078	3937.687891	16.808243	-0.050259	3.427122
260.245731	3929.668629	16.813248	-0.050184	3.423810
260.255041	3921.719263	16.818253	-0.050181	3.420537
260.299808	3913.707201	16.823258	-0.050183	3.417236
260.409045	3905.711147	16.828263	-0.050198	3.413941
260.348903	3897.709606	16.833267	-0.050182	3.410634
260.295642	3889.703209	16.838272	-0.050166	3.407323
260.250966	3881.743880	16.843277	-0.050153	3.404028
260.150796	3873.763765	16.848282	-0.050129	3.400719
259.950625	3865.836717	16.853287	-0.050086	3.397426
260.095203	3857.773497	16.858291	-0.050108	3.394085
259.864238	3849.685117	16.863296	-0.050059	3.390717
259.907363	3841.730384	16.868301	-0.050062	3.387410
259.983750	3833.733362	16.873306	-0.050071	3.384084
259.916734	3825.801996	16.878311	-0.050053	3.380778
259.849175	3817.831332	16.883315	-0.050035	3.377451
259.857939	3809.806007	16.888320	-0.050031	3.374101
259.797575	3801.807984	16.893325	-0.050014	3.370757
259.584280	3793.820550	16.898330	-0.049969	3.367408
259.601986	3785.837789	16.903335	-0.049967	3.364067
259.799350	3777.865412	16.908339	-0.049998	3.360732
259.577900	3769.865468	16.913344	-0.049952	3.357368
259.614930	3761.870695	16.918349	-0.049953	3.354012
259.699113	3753.854601	16.923354	-0.049964	3.350645
259.651319	3745.865370	16.928359	-0.049949	3.347281
259.662879	3737.902012	16.933363	-0.049946	3.343927
259.604574	3729.892033	16.938368	-0.049930	3.340548
259.623331	3721.916007	16.943373	-0.049928	3.337182
259.500284	3713.922741	16.948378	-0.049900	3.333800
259.609812	3705.895896	16.953383	-0.049915	3.330409
259.651663	3697.938394	16.958387	-0.049917	3.327042
259.372215	3689.944287	16.963392	-0.049860	3.323644
259.426883	3681.984956	16.968397	-0.049864	3.320269
259.384694	3674.011387	16.973402	-0.049851	3.316882
259.173038	3665.982444	16.978407	-0.049806	3.313460
259.133124	3657.964999	16.983411	-0.049793	3.310047
259.110395	3649.970436	16.988416	-0.049784	3.306641
259.077526	3642.013568	16.993421	-0.049772	3.303246
258.924498	3634.015683	16.998426	-0.049738	3.299827
258.762533	3626.056176	17.003431	-0.049703	3.296419
258.941593	3618.036473	17.008435	-0.049731	3.292996
258.822924	3610.012428	17.013440	-0.049703	3.289555
258.777460	3602.076148	17.018445	-0.049689	3.286152
258.847672	3594.077320	17.023450	-0.049697	3.282722
258.856747	3586.082905	17.028455	-0.049693	3.279289
258.804263	3578.138727	17.033459	-0.049678	3.275871
258.731325	3570.088014	17.038464	-0.049659	3.272402
258.832606	3562.082160	17.043469	-0.049673	3.268957
258.692302	3554.101671	17.048474	-0.049641	3.265509
258.538560	3546.143196	17.053479	-0.049607	3.262066
258.574262	3538.153473	17.058483	-0.049608	3.258614
258.402957	3530.152985	17.063488	-0.049571	3.255145
258.650135	3522.139911	17.068493	-0.049612	3.251683
258.661061	3514.133283	17.073498	-0.049608	3.248212
258.546058	3506.161940	17.078503	-0.049582	3.244747
258.370345	3498.245716	17.083507	-0.049543	3.241299
258.322465	3490.243665	17.088512	-0.049529	3.237816
258.291712	3482.258691	17.093517	-0.049518	3.234337
258.191522	3474.187166	17.098522	-0.049494	3.230814
258.118968	3466.191265	17.103527	-0.049475	3.227321
258.267342	3458.211251	17.108531	-0.049497	3.223841
258.218218	3450.220486	17.113536	-0.049483	3.220343
258.230986	3442.256134	17.118541	-0.049480	3.216856
258.190123	3434.255634	17.123546	-0.049467	3.213347
258.099453	3426.240863	17.128551	-0.049444	3.209826
258.011687	3418.309947	17.133555	-0.049423	3.206339
257.835254	3410.307418	17.138560	-0.049384	3.202812
258.068772	3402.342228	17.143565	-0.049422	3.199314
257.810516	3394.386371	17.148570	-0.049369	3.195797
257.897672	3386.344275	17.153575	-0.049380	3.192252
257.749439	3378.375921	17.158579	-0.049347	3.188725
257.696287	3370.360798	17.163584	-0.049332	3.185179
257.637768	3362.427034	17.168589	-0.049315	3.181664
257.383761	3354.454667	17.173594	-0.049263	3.178119
257.437355	3346.405470	17.178599	-0.049267	3.174550
257.405583	3338.419892	17.183603	-0.049256	3.171001
257.445753	3330.411064	17.188608	-0.049258	3.167441
257.579838	3322.426662	17.193613	-0.049277	3.163892
257.282562	3314.481095	17.198618	-0.049217	3.160337
257.149982	3306.524416	17.203623	-0.049187	3.156781
257.359317	3298.470139	17.208627	-0.049220	3.153192
257.222639	3290.456600	17.213632	-0.049189	3.149602
257.187631	3282.482050	17.218637	-0.049177	3.146030
257.174030	3274.506825	17.223642	-0.049170	3.142454
257.020454	3266.538436	17.228647	-0.049136	3.138871
257.140718	3258.565487	17.233651	-0.049153	3.135295
256.875580	3250.547299	17.238656	-0.049098	3.131676
257.100798	3242.573244	17.243661	-0.049134	3.128095
256.876283	3234.573112	17.248666	-0.049087	3.124478
256.734857	3226.628735	17.253671	-0.049055	3.120886
256.830942	3218.647895	17.258675	-0.049068	3.117284
256.795246	3210.652795	17.263680	-0.049056	3.113665
256.962873	3202.621252	17.268685	-0.049082	3.110035
256.679540	3194.659189	17.273690	-0.049023	3.106412
256.722582	3186.660839	17.278695	-0.049026	3.102782
256.741348	3178.689365	17.283699	-0.049024	3.099160
256.735165	3170.698171	17.288704	-0.049018	3.095523
256.945140	3162.670646	17.293709	-0.049051	3.091875
256.539416	3154.736478	17.298714	-0.048970	3.088238
256.413184	3146.754928	17.303719	-0.048942	3.084587
256.506464	3138.789332	17.308723	-0.048953	3.080949
256.478480	3130.791553	17.313728	-0.048943	3.077287
256.282644	3122.793820	17.318733	-0.048901	3.073612
256.394175	3114.733658	17.323738	-0.048916	3.069919
256.292478	3106.748361	17.328743	-0.048892	3.066245
256.314407	3098.808892	17.333747	-0.048891	3.062594
256.032362	3090.838191	17.338752	-0.048833	3.058910
256.102241	3082.866848	17.343757	-0.048840	3.055238
256.173982	3074.827813	17.348762	-0.048848	3.051531
256.233793	3066.836196	17.353767	-0.048854	3.047840
256.161106	3058.900941	17.358771	-0.048835	3.044164
256.209087	3050.906268	17.363776	-0.048839	3.040463
256.105573	3042.983407	17.368781	-0.048814	3.036782
256.066874	3034.933153	17.373786	-0.048801	3.033042
256.093737	3026.931664	17.378791	-0.048801	3.029322
256.188068	3018.965133	17.383795	-0.048813	3.025617
255.854696	3011.010766	17.388800	-0.048746	3.021893
255.980810	3003.035734	17.393805	-0.048764	3.018177
255.969611	2995.032763	17.398810	-0.048756	3.014437
255.672943	2987.048342	17.403815	-0.048696	3.010686
255.859680	2979.065843	17.408819	-0.048725	3.006956
255.515586	2971.105814	17.413824	-0.048656	3.003205
255.783156	2963.090058	17.418829	-0.048700	2.999453
255.526032	2955.162202	17.423834	-0.048647	2.995713
255.516817	2947.124038	17.428839	-0.048640	2.991928
255.718892	2939.108057	17.433843	-0.048672	2.988159
255.568459	2931.109799	17.438848	-0.048638	2.984376
255.589414	2923.179437	17.443853	-0.048637	2.980629
255.514637	2915.234961	17.448858	-0.048618	2.976865
255.432291	2907.222363	17.453863	-0.048597	2.973065
255.348092	2899.207760	17.458867	-0.048576	2.969258
255.266981	2891.224166	17.463872	-0.048555	2.965461
255.253080	2883.289538	17.468877	-0.048547	2.961687
255.354530	2875.287766	17.473882	-0.048561	2.957881
255.317492	2867.302010	17.478887	-0.048549	2.954071
255.455930	2859.293906	17.483891	-0.048569	2.950254
255.172298	2851.327400	17.488896	-0.048511	2.946431
255.047733	2843.356101	17.493901	-0.048482	2.942608
255.186027	2835.366688	17.498906	-0.048503	2.938785
254.956576	2827.414596	17.503911	-0.048454	2.934957
254.904524	2819.421864	17.508915	-0.048439	2.931112
254.884964	2811.427673	17.513920	-0.048430	2.927264
254.861251	2803.467121	17.518925	-0.048421	2.923427
254.659320	2795.496466	17.523930	-0.048378	2.919570
254.601299	2787.525180	17.528935	-0.048361	2.915716
254.763176	2779.459683	17.533939	-0.048386	2.911823
254.577685	2771.447648	17.538944	-0.048346	2.907931
254.503172	2763.487579	17.543949	-0.048327	2.904066
254.558748	2755.538546	17.548954	-0.048332	2.900208
254.432003	2747.561230	17.553959	-0.048303	2.896321
254.472435	2739.590247	17.558963	-0.048305	2.892441
254.271408	2731.585752	17.563968	-0.048262	2.888526
254.451894	2723.600232	17.568973	-0.048290	2.884636
254.457135	2715.660874	17.573978	-0.048286	2.880754
254.183896	2707.711703	17.578983	-0.048230	2.876846
254.439919	2699.664014	17.583987	-0.048272	2.872914
254.175777	2691.698198	17.588992	-0.048217	2.868988
254.036886	2683.717949	17.593997	-0.048186	2.865057
254.241321	2675.761453	17.599002	-0.048219	2.861151
254.167824	2667.772981	17.604007	-0.048200	2.857208
254.030481	2659.814785	17.609011	-0.048169	2.853271
254.011706	2651.805659	17.614016	-0.048160	2.849310
254.059700	2643.822177	17.619021	-0.048163	2.845360
253.938848	2635.890297	17.624026	-0.048136	2.841421
253.826679	2627.903144	17.629031	-0.048109	2.837449
253.937529	2619.917548	17.634035	-0.048125	2.833485
253.862203	2611.905382	17.639040	-0.048105	2.829492
253.627505	2603.947795	17.644045	-0.048056	2.825511
253.509615	2595.985692	17.649050	-0.048029	2.821529
253.596024	2587.984660	17.654055	-0.048039	2.817533
253.605819	2580.001853	17.659059	-0.048036	2.813537
253.455163	2571.999671	17.664064	-0.048002	2.809515
253.637636	2564.037775	17.669069	-0.048031	2.805528
253.449681	2556.101279	17.674074	-0.047991	2.801526
253.146539	2548.139970	17.679079	-0.047929	2.797499
253.450103	2540.117613	17.684083	-0.047980	2.793471
253.110116	2532.136772	17.689088	-0.047911	2.789421
253.072491	2524.161600	17.694093	-0.047899	2.785385
253.238502	2516.179870	17.699098	-0.047924	2.781352
253.269100	2508.196490	17.704103	-0.047925	2.777305
253.319443	2500.230411	17.709107	-0.047929	2.773261
253.117274	2492.245334	17.714112	-0.047886	2.769187
253.154676	2484.271632	17.719117	-0.047887	2.765127
253.209662	2476.303889	17.724122	-0.047892	2.761064
253.030665	2468.352730	17.729127	-0.047853	2.756991
253.116623	2460.331044	17.734131	-0.047864	2.752891
252.949387	2452.298134	17.739136	-0.047827	2.748764
252.797778	2444.336318	17.744141	-0.047794	2.744668
252.727863	2436.417475	17.749146	-0.047775	2.740594
252.662759	2428.441400	17.754151	-0.047758	2.736483
252.745290	2420.455598	17.759155	-0.047768	2.732371
252.720261	2412.459507	17.764160	-0.047758	2.728241
252.880502	2404.472194	17.769165	-0.047782	2.724120
252.632113	2396.556418	17.774170	-0.047731	2.720005
252.414048	2388.607040	17.779175	-0.047685	2.715868
252.723589	2380.583394	17.784179	-0.047737	2.711719
252.702030	2372.583922	17.789184	-0.047727	2.707555
252.559455	2364.631037	17.794189	-0.047695	2.703402
252.586250	2356.671299	17.799194	-0.047695	2.699249
252.619422	2348.693186	17.804199	-0.047696	2.695081
252.507253	2340.735973	17.809203	-0.047670	2.690908
252.150463	2332.765366	17.814208	-0.047598	2.686706
252.354670	2324.784150	17.819213	-0.047630	2.682528
252.185954	2316.837284	17.824218	-0.047594	2.678337
252.127544	2308.849894	17.829223	-0.047577	2.674126
252.148105	2300.837146	17.834227	-0.047576	2.669899
252.234860	2292.857352	17.839232	-0.047586	2.665688
252.132729	2284.913726	17.844237	-0.047562	2.661476
251.887752	2276.966039	17.849242	-0.047511	2.657247
251.959201	2268.965433	17.854247	-0.047519	2.653003
252.067814	2260.983005	17.859251	-0.047534	2.648765
251.864678	2253.012288	17.864256	-0.047491	2.644505
252.044272	2245.064518	17.869261	-0.047519	2.640277
252.061792	2237.090067	17.874266	-0.047517	2.636016
251.843056	2229.107783	17.879271	-0.047470	2.631729
251.702485	2221.158656	17.884275	-0.047439	2.627457
251.924828	2213.152988	17.889280	-0.047475	2.623173
251.627924	2205.228321	17.894285	-0.047414	2.618890
251.662895	2197.245530	17.899290	-0.047415	2.614591
251.564567	2189.255696	17.904295	-0.047392	2.610273
251.593079	2181.299428	17.909299	-0.047392	2.605973
251.381747	2173.350141	17.914304	-0.047347	2.601655
251.568001	2165.378374	17.919309	-0.047376	2.597344
251.442858	2157.332608	17.924314	-0.047347	2.592964
251.411135	2149.242961	17.929319	-0.047336	2.588559
251.441708	2141.311500	17.934323	-0.047336	2.584238
251.470247	2133.354980	17.939328	-0.047336	2.579895
251.219169	2125.451555	17.944333	-0.047284	2.575555
251.266826	2117.489250	17.949338	-0.047288	2.571195
251.398176	2109.492916	17.954343	-0.047307	2.566816
251.405154	2101.551106	17.959347	-0.047303	2.562450
251.098303	2093.639298	17.964352	-0.047240	2.558072
250.992103	2085.682998	17.969357	-0.047215	2.553675
251.052041	2077.677607	17.974362	-0.047221	2.549255
251.042788	2069.695134	17.979367	-0.047214	2.544836
250.968661	2061.767129	17.984371	-0.047195	2.540434
250.929465	2053.784156	17.989376	-0.047182	2.535997
250.783757	2045.827930	17.994381	-0.047149	2.531559
250.708243	2037.869490	17.999386	-0.047130	2.527117
250.583139	2029.895125	18.004391	-0.047101	2.522655
250.654222	2021.954112	18.009395	-0.047109	2.518218
250.400010	2013.995352	18.014400	-0.047056	2.513740
250.344510	2005.992309	18.019405	-0.047041	2.509242
250.441447	1998.007577	18.024410	-0.047053	2.504759
250.302031	1990.072551	18.029415	-0.047022	2.500278
250.345070	1982.097588	18.034419	-0.047025	2.495779
250.372956	1974.103076	18.039424	-0.047024	2.491261
250.286753	1966.152145	18.044429	-0.047003	2.486750
250.201842	1958.221290	18.049434	-0.046982	2.482243
250.187240	1950.254878	18.054439	-0.046974	2.477712
250.319060	1942.273851	18.059443	-0.046993	2.473176
250.053064	1934.321245	18.064448	-0.046938	2.468618
250.052647	1926.343907	18.069453	-0.046932	2.464057
249.941979	1918.406910	18.074458	-0.046906	2.459503
249.957655	1910.442587	18.079463	-0.046904	2.454934
250.051318	1902.457622	18.084467	-0.046916	2.450350
249.929399	1894.508800	18.089472	-0.046888	2.445763
249.828186	1886.579806	18.094477	-0.046864	2.441180
249.645378	1878.662209	18.099482	-0.046824	2.436588
249.745155	1870.584528	18.104487	-0.046838	2.431917
249.665906	1862.622794	18.109491	-0.046817	2.427290
249.549493	1854.657599	18.114496	-0.046790	2.422649
249.507672	1846.728634	18.119501	-0.046777	2.418027
249.567077	1838.755736	18.124506	-0.046783	2.413377
249.391836	1830.779464	18.129511	-0.046745	2.408699
249.623211	1822.812866	18.134515	-0.046783	2.404049
249.625550	1814.879293	18.139520	-0.046778	2.399391
249.671720	1806.922923	18.144525	-0.046781	2.394714
249.502351	1798.967996	18.149530	-0.046744	2.390012
249.390860	1791.003916	18.154535	-0.046718	2.385300
249.460803	1783.074282	18.159539	-0.046725	2.380613
249.262207	1775.131280	18.164544	-0.046683	2.375888
249.269104	1767.145347	18.169549	-0.046679	2.371144
249.187118	1759.202277	18.174554	-0.046658	2.366409
249.051834	1751.254358	18.179559	-0.046628	2.361657
249.009926	1743.327654	18.184563	-0.046615	2.356916
249.198574	1735.315712	18.189568	-0.046644	2.352133
248.997518	1727.349553	18.194573	-0.046601	2.347336
248.813010	1719.431010	18.199578	-0.046562	2.342559
248.652871	1711.473665	18.204583	-0.046527	2.337751
248.735370	1703.512201	18.209587	-0.046537	2.332951
248.678872	1695.547321	18.214592	-0.046521	2.328127
248.611724	1687.593742	18.219597	-0.046503	2.323299
248.633969	1679.676609	18.224602	-0.046502	2.318490
248.548217	1671.701508	18.229607	-0.046480	2.313627
248.627645	1663.734155	18.234611	-0.046490	2.308773
248.543085	1655.762618	18.239616	-0.046468	2.303892
248.473252	1647.842901	18.244621	-0.046450	2.299033
248.308367	1639.916711	18.249626	-0.046414	2.294153
248.251474	1631.930030	18.254631	-0.046398	2.289233
248.467890	1623.963326	18.259635	-0.046433	2.284339
248.490892	1616.017023	18.264640	-0.046432	2.279430
248.321073	1608.093313	18.269645	-0.046395	2.274508
248.281780	1600.063021	18.274650	-0.046382	2.269521
248.215978	1592.099444	18.279655	-0.046365	2.264561
248.132585	1584.198809	18.284659	-0.046344	2.259629
248.075700	1576.262117	18.289664	-0.046328	2.254665
247.847699	1568.322170	18.294669	-0.046280	2.249674
247.902031	1560.361879	18.299674	-0.046285	2.244683
247.806274	1552.430768	18.304679	-0.046261	2.239687
248.049493	1544.471268	18.309683	-0.046301	2.234691
247.623420	1536.534947	18.314688	-0.046217	2.229639
247.575571	1528.569058	18.319693	-0.046202	2.224591
247.709127	1520.630945	18.324698	-0.046222	2.219565
247.617042	1512.691182	18.329703	-0.046199	2.214507
247.785149	1504.724435	18.334707	-0.046225	2.209442
247.660177	1496.794672	18.339712	-0.046197	2.204364
247.677033	1488.860078	18.344717	-0.046194	2.199284
247.557265	1480.948037	18.349722	-0.046167	2.194194
247.387584	1472.962383	18.354727	-0.046130	2.189040
247.528580	1465.001904	18.359731	-0.046151	2.183918
247.515642	1457.076757	18.364736	-0.046143	2.178793
247.337435	1449.139353	18.369741	-0.046104	2.173633
247.216819	1441.207435	18.374746	-0.046077	2.168470
247.180844	1433.262548	18.379751	-0.046064	2.163293
247.286981	1425.328597	18.384755	-0.046079	2.158125
247.238583	1417.377486	18.389760	-0.046064	2.152918
247.283249	1409.401647	18.394765	-0.046067	2.147692
247.111546	1401.507231	18.399770	-0.046030	2.142485
246.886918	1393.584344	18.404775	-0.045983	2.137243
247.049246	1385.621934	18.409779	-0.046008	2.131997
246.839413	1377.700718	18.414784	-0.045963	2.126731
246.829336	1369.766739	18.419789	-0.045956	2.121463
246.776525	1361.856277	18.424794	-0.045941	2.116192
246.559165	1353.862660	18.429799	-0.045895	2.110837
246.385458	1345.934432	18.434803	-0.045857	2.105517
246.304002	1337.996960	18.439808	-0.045837	2.100186
246.438376	1330.049790	18.444813	-0.045856	2.094855
246.312464	1322.133907	18.449818	-0.045828	2.089507
246.372259	1314.162010	18.454823	-0.045833	2.084125
246.296413	1306.268343	18.459827	-0.045814	2.078769
246.230746	1298.333444	18.464832	-0.045796	2.073372
246.213028	1290.389120	18.469837	-0.045788	2.067960
246.100852	1282.478702	18.474842	-0.045761	2.062547
246.146352	1274.533943	18.479847	-0.045765	2.057112
246.080691	1266.619594	18.484851	-0.045747	2.051672
245.880832	1258.693403	18.489856	-0.045704	2.046196
246.011513	1250.753343	18.494861	-0.045723	2.040729
245.831404	1242.865270	18.499866	-0.045685	2.035252
245.667136	1234.905229	18.504871	-0.045649	2.029712
245.812864	1226.962320	18.509875	-0.045670	2.024200
245.734280	1219.035369	18.514880	-0.045650	2.018661
245.798702	1211.096147	18.519885	-0.045657	2.013113
245.661417	1203.188815	18.524890	-0.045626	2.007552
245.627180	1195.263389	18.529895	-0.045614	2.001973
245.444439	1187.379002	18.534899	-0.045575	1.996391
245.428468	1179.422155	18.539904	-0.045567	1.990760
245.314771	1171.504543	18.544909	-0.045540	1.985131
245.575812	1163.565240	18.549914	-0.045583	1.979510
245.402892	1155.659239	18.554919	-0.045546	1.973851
245.215353	1147.753375	18.559923	-0.045506	1.968173
245.210122	1139.834493	18.564928	-0.045499	1.962490
245.072110	1131.940218	18.569933	-0.045468	1.956793
245.140939	1123.969549	18.574938	-0.045476	1.951047
245.122184	1116.014754	18.579943	-0.045467	1.945286
245.016080	1108.135708	18.584947	-0.045442	1.939554
244.772115	1100.235913	18.589952	-0.045391	1.933774
244.806312	1092.294517	18.594957	-0.045392	1.927977
244.802471	1084.390133	18.599962	-0.045386	1.922185
244.656030	1076.493758	18.604967	-0.045353	1.916366
244.514189	1068.585449	18.609971	-0.045321	1.910521
244.590771	1060.645371	18.614976	-0.045330	1.904659
244.501936	1052.750312	18.619981	-0.045308	1.898793
244.613160	1044.837790	18.624986	-0.045324	1.892919
244.696719	1036.887701	18.629991	-0.045334	1.886996
244.618062	1029.011313	18.634995	-0.045314	1.881090
244.481297	1021.134720	18.640000	-0.045283	1.875159
244.438935	1013.188042	18.645005	-0.045270	1.869168
244.498076	1005.275668	18.650010	-0.045276	1.863194
244.269056	997.402450	18.655015	-0.045228	1.857198
244.261591	989.485441	18.660019	-0.045221	1.851175
244.316303	981.558697	18.665024	-0.045226	1.845132
244.163870	973.705114	18.670029	-0.045192	1.839100
243.817356	965.845152	18.675034	-0.045122	1.833021
243.942257	957.887201	18.680039	-0.045140	1.826902
243.892473	950.002635	18.685043	-0.045126	1.820799
243.657577	942.131705	18.690048	-0.045076	1.814663
243.732108	934.208331	18.695053	-0.045085	1.808503
243.889536	926.298820	18.700058	-0.045109	1.802343
243.553136	918.453299	18.705063	-0.045041	1.796151
243.477581	910.514014	18.710067	-0.045022	1.789897
243.489869	902.604856	18.715072	-0.045019	1.783655
243.518001	894.704538	18.720077	-0.045018	1.777399
243.414001	886.830770	18.725082	-0.044994	1.771127
243.323689	878.938477	18.730087	-0.044972	1.764819
243.388057	871.059837	18.735091	-0.044978	1.758519
243.143479	863.200192	18.740096	-0.044927	1.752173
242.934217	855.325814	18.745101	-0.044883	1.745796
242.995701	847.440073	18.750106	-0.044889	1.739420
242.973623	839.543877	18.755111	-0.044880	1.733002
242.902104	831.664219	18.760115	-0.044861	1.726568
243.070559	823.769951	18.765120	-0.044887	1.720128
242.967039	815.908955	18.770125	-0.044863	1.713656
242.873223	808.029696	18.775130	-0.044840	1.707146
242.751620	800.147651	18.780135	-0.044812	1.700605
242.845629	792.273377	18.785139	-0.044824	1.694073
242.736620	784.393635	18.790144	-0.044798	1.687485
242.596730	776.549421	18.795149	-0.044767	1.680897
242.758417	768.672675	18.800154	-0.044792	1.674295
242.328495	760.840569	18.805159	-0.044706	1.667626
242.407441	752.951225	18.810163	-0.044716	1.660950
242.256613	745.117931	18.815168	-0.044682	1.654264
242.296712	737.219441	18.820173	-0.044685	1.647520
242.207633	729.394120	18.825178	-0.044663	1.640794
241.922606	721.553175	18.830183	-0.044604	1.634000
241.962436	713.622740	18.835187	-0.044606	1.627145
241.969424	705.760637	18.840192	-0.044602	1.620316
241.807313	697.932808	18.845197	-0.044567	1.613464
241.790063	690.068160	18.850202	-0.044558	1.606571
241.825924	682.212751	18.855207	-0.044560	1.599664
241.726981	674.387456	18.860211	-0.044536	1.592734
241.771964	666.508151	18.865216	-0.044539	1.585747
241.721687	658.681949	18.870221	-0.044524	1.578762
241.623553	650.857557	18.875226	-0.044501	1.571742
241.455117	643.021509	18.880231	-0.044464	1.564668
241.480962	635.191130	18.885235	-0.044464	1.557597
241.391388	627.346092	18.890240	-0.044442	1.550462
241.134003	619.534159	18.895245	-0.044388	1.543300
241.169275	611.697257	18.900250	-0.044390	1.536125
241.190066	603.836091	18.905255	-0.044388	1.528892
241.253610	596.005734	18.910259	-0.044395	1.521660
241.085718	588.216455	18.915264	-0.044358	1.514396
241.041485	580.373778	18.920269	-0.044345	1.507066
240.857127	572.592092	18.925274	-0.044305	1.499736
240.778736	564.763215	18.930279	-0.044285	1.492342
240.750185	556.942471	18.935283	-0.044275	1.484926
240.695760	549.152545	18.940288	-0.044259	1.477498
240.561055	541.301383	18.945293	-0.044229	1.469962
240.833358	533.445402	18.950298	-0.044274	1.462446
240.689172	525.664830	18.955303	-0.044242	1.454899
240.632591	517.865765	18.960307	-0.044226	1.447308
240.491653	510.096307	18.965312	-0.044195	1.439692
240.408436	502.310173	18.970317	-0.044174	1.432029
240.332838	494.517957	18.975322	-0.044155	1.424319
240.246163	486.735570	18.980327	-0.044133	1.416576
240.204175	478.947646	18.985331	-0.044120	1.408792
240.187314	471.173887	18.990336	-0.044112	1.400983
239.995778	463.421938	18.995341	-0.044071	1.393123
240.063425	455.605829	19.000346	-0.044078	1.385197
239.983877	447.837986	19.005351	-0.044058	1.377250
240.030064	440.056299	19.010355	-0.044062	1.369263
239.763249	432.337482	19.015360	-0.044007	1.361241
239.645891	424.593789	19.020365	-0.043980	1.353172
239.625664	416.831270	19.025370	-0.043971	1.345051
239.383285	409.099553	19.030375	-0.043920	1.336874
239.452508	401.323256	19.035379	-0.043928	1.328655
239.462996	393.576475	19.040384	-0.043924	1.320406
239.212107	385.817183	19.045389	-0.043873	1.312044
239.271357	377.997120	19.050394	-0.043878	1.303619
239.044967	370.296813	19.055399	-0.043831	1.295217
238.951165	362.582171	19.060403	-0.043808	1.286769
238.814300	354.891543	19.065408	-0.043778	1.278284
238.734690	347.175054	19.070413	-0.043757	1.269724
238.807995	339.448855	19.075418	-0.043766	1.261124
238.616102	331.772784	19.080423	-0.043725	1.252471
238.644091	324.063177	19.085427	-0.043725	1.243762
238.500173	316.396630	19.090432	-0.043693	1.235007
238.496146	308.672422	19.095437	-0.043687	1.226150
238.400710	301.013014	19.100442	-0.043664	1.217287
238.378902	293.320280	19.105447	-0.043655	1.208334
238.428889	285.643233	19.110451	-0.043659	1.199346
238.104266	278.033187	19.115456	-0.043593	1.190295
238.113345	270.352085	19.120461	-0.043590	1.181158
238.332302	262.673720	19.125466	-0.043625	1.171995
238.027912	255.072967	19.130471	-0.043564	1.162746
237.929660	247.446903	19.135475	-0.043540	1.153435
237.841994	239.790394	19.140480	-0.043519	1.144013
237.651665	232.191359	19.145485	-0.043478	1.134562
237.651908	224.568415	19.150490	-0.043473	1.125043
237.576777	216.972061	19.155495	-0.043454	1.115459
237.283966	209.412647	19.160499	-0.043394	1.105792
237.281440	201.821209	19.165504	-0.043389	1.096063
237.224673	194.232553	19.170509	-0.043373	1.086238
237.090171	186.693906	19.175514	-0.043343	1.076371
236.820315	179.144110	19.180519	-0.043287	1.066367
236.724494	171.601947	19.185523	-0.043264	1.056318
237.018856	163.996880	19.190528	-0.043314	1.046180
236.846282	156.500908	19.195533	-0.043277	1.035980
236.643317	149.009340	19.200538	-0.043234	1.025678
236.579034	141.505919	19.205543	-0.043217	1.015288
236.583284	134.003200	19.210547	-0.043213	1.004809
236.331212	126.559461	19.215552	-0.043161	0.994239
236.355862	119.040204	19.220557	-0.043160	0.983517
236.298033	111.594379	19.225562	-0.043144	0.972762
236.084017	104.176099	19.230567	-0.043099	0.961887
235.887431	96.781601	19.235571	-0.043058	0.950927
235.849304	89.365200	19.240576	-0.043046	0.939848
235.719597	81.976126	19.245581	-0.043017	0.928654
235.676183	74.610698	19.250586	-0.043003	0.917383
235.659424	67.226955	19.255591	-0.042995	0.905951
235.684988	60.109213	19.260595	-0.042995	0.894804