Fri Mar 12 11:27:16 2021


Number of Points = 3627

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
-0.019356	0.025644	0.000000	0.000019	0.718623
-0.010874	-0.044226	0.005005	0.000017	0.718488
0.160154	-0.142798	0.010010	-0.000014	0.718353
0.003078	-0.117007	0.015014	0.000015	0.718348
0.128802	-0.141428	0.020019	-0.000008	0.718344
0.226891	-0.155196	0.025024	-0.000026	0.718351
0.017763	-0.121953	0.030029	0.000013	0.718343
0.020288	-0.119965	0.035034	0.000013	0.718347
-0.083258	-0.101693	0.040038	0.000032	0.718347
0.040307	-0.123358	0.045043	0.000009	0.718347
0.052103	-0.121085	0.050048	0.000007	0.718355
0.058406	-0.127160	0.055053	0.000006	0.718345
0.222996	-0.153603	0.060058	-0.000024	0.718351
0.282967	-0.165562	0.065062	-0.000035	0.718348
-0.008430	-0.115769	0.070067	0.000019	0.718343
-0.085652	-0.109299	0.075072	0.000034	0.718329
-0.170637	-0.256673	0.080077	0.000050	0.718007
-0.076148	-0.267985	0.085082	0.000032	0.718018
-0.066514	-0.271412	0.090086	0.000031	0.718014
-0.023389	-0.280212	0.095091	0.000023	0.718012
0.025330	-0.285426	0.100096	0.000014	0.718018
-0.083056	-0.270123	0.105101	0.000034	0.718010
0.187002	-0.372505	0.110106	-0.000016	0.717903
-0.061736	-0.427093	0.115110	0.000030	0.717707
-0.098247	-0.423129	0.120115	0.000037	0.717702
-0.077379	-0.422910	0.125120	0.000034	0.717709
-0.007251	-0.441100	0.130125	0.000021	0.717698
0.127438	-0.510821	0.135130	-0.000004	0.717607
0.071148	-0.614643	0.140134	0.000007	0.717381
0.028234	-0.610366	0.145139	0.000015	0.717375
0.201228	-0.637088	0.150144	-0.000017	0.717382
0.204799	-0.669899	0.155149	-0.000018	0.717318
0.079921	-0.765995	0.160154	0.000006	0.717084
0.274545	-0.799373	0.165158	-0.000030	0.717086
0.124188	-0.777060	0.170163	-0.000002	0.717077
0.151366	-0.877959	0.175168	-0.000007	0.716887
0.043510	-0.927099	0.180173	0.000013	0.716751
-0.064369	-0.906002	0.185178	0.000033	0.716755
-0.112334	-0.936031	0.190182	0.000043	0.716678
-0.065050	-1.062845	0.195187	0.000034	0.716443
-0.016381	-1.066876	0.200192	0.000025	0.716452
-0.124162	-1.067434	0.205197	0.000045	0.716413
-0.087630	-1.215415	0.210202	0.000039	0.716132
0.093062	-1.248482	0.215206	0.000005	0.716130
-0.037360	-1.256540	0.220211	0.000030	0.716068
-0.103742	-1.336186	0.225216	0.000042	0.715886
0.021347	-1.363522	0.230221	0.000019	0.715876
-0.071470	-1.429851	0.235226	0.000037	0.715712
-0.127186	-1.503911	0.240230	0.000047	0.715545
0.022388	-1.533718	0.245235	0.000020	0.715538
0.177395	-1.702278	0.250240	-0.000009	0.715258
-0.163928	-1.657617	0.255245	0.000055	0.715226
0.004253	-1.767297	0.260250	0.000023	0.715068
-0.078023	-1.832223	0.265254	0.000039	0.714909
-0.254336	-1.827096	0.270259	0.000072	0.714857
-0.168685	-1.964729	0.275264	0.000056	0.714614
-0.421898	-1.924583	0.280269	0.000104	0.714604
-0.404280	-2.064395	0.285274	0.000101	0.714332
-0.356405	-2.100050	0.290278	0.000092	0.714278
-0.433890	-2.179254	0.295283	0.000106	0.714093
-0.383386	-2.247106	0.300288	0.000097	0.713976
-0.570726	-2.282705	0.305293	0.000132	0.713838
-0.483802	-2.389573	0.310298	0.000116	0.713656
-0.403317	-2.449345	0.315302	0.000101	0.713566
-0.681523	-2.503485	0.320307	0.000153	0.713359
-0.590156	-2.556702	0.325312	0.000137	0.713285
-3.277258	-2.209879	0.330317	0.000637	0.713023
-3.396655	-2.186577	0.335322	0.000659	0.713026
-4.080381	-2.090455	0.340326	0.000787	0.712975
-4.493424	-2.151798	0.345331	0.000864	0.712706
-4.285568	-2.183944	0.350336	0.000825	0.712715
-5.148975	-2.034349	0.355341	0.000986	0.712707
-4.966221	-2.162684	0.360346	0.000952	0.712516
-5.616400	-2.109352	0.365350	0.001073	0.712391
-5.559914	-2.123896	0.370355	0.001063	0.712382
-5.162161	-2.188941	0.375360	0.000989	0.712393
-5.723696	-2.163419	0.380365	0.001094	0.712244
-6.553554	-2.092262	0.385370	0.001249	0.712091
-5.973513	-2.196764	0.390374	0.001141	0.712089
-6.684257	-2.072363	0.395379	0.001273	0.712084
-6.571889	-2.090830	0.400384	0.001252	0.712087
-6.639825	-2.243790	0.405389	0.001265	0.711757
-7.307698	-2.121347	0.410394	0.001390	0.711764
-7.672440	-2.055739	0.415398	0.001458	0.711765
-7.060983	-2.167015	0.420403	0.001344	0.711760
-7.132647	-2.182247	0.425408	0.001358	0.711704
-8.529958	-2.061289	0.430413	0.001618	0.711448
-7.958359	-2.160417	0.435418	0.001512	0.711453
-8.163838	-2.122052	0.440422	0.001550	0.711456
-8.477102	-2.067141	0.445427	0.001609	0.711454
-8.091787	-2.132526	0.450432	0.001537	0.711461
-8.553739	-2.174128	0.455437	0.001623	0.711213
-9.372434	-2.065252	0.460442	0.001776	0.711139
-8.976582	-2.136742	0.465446	0.001702	0.711137
-8.806193	-2.166647	0.470451	0.001671	0.711137
-9.004243	-2.126946	0.475456	0.001708	0.711146
-9.231362	-2.099861	0.480461	0.001750	0.711119
-9.558882	-2.165745	0.485466	0.001811	0.710871
-9.627918	-2.153023	0.490470	0.001824	0.710871
-9.885364	-2.108447	0.495475	0.001872	0.710868
-9.622712	-2.151353	0.500480	0.001824	0.710876
-9.692410	-2.142541	0.505485	0.001837	0.710868
-9.946036	-2.176089	0.510490	0.001884	0.710711
-10.800682	-2.110095	0.515494	0.002043	0.710538
-10.481726	-2.170892	0.520499	0.001984	0.710530
-10.705549	-2.126483	0.525504	0.002026	0.710539
-11.039991	-2.071701	0.530509	0.002088	0.710529
-10.917513	-2.091155	0.535514	0.002066	0.710533
-10.642051	-2.157449	0.540518	0.002015	0.710499
-11.584048	-2.132734	0.545523	0.002190	0.710212
-11.558685	-2.130585	0.550528	0.002186	0.710225
-11.913365	-2.073052	0.555533	0.002252	0.710214
-11.462994	-2.151996	0.560538	0.002168	0.710216
-11.576786	-2.131298	0.565542	0.002189	0.710217
-11.752684	-2.104962	0.570547	0.002222	0.710206
-11.518743	-2.245860	0.575552	0.002179	0.710008
-12.924365	-2.056671	0.580557	0.002441	0.709885
-12.813235	-2.072466	0.585562	0.002420	0.709893
-12.426729	-2.140927	0.590566	0.002348	0.709893
-12.662732	-2.100948	0.595571	0.002392	0.709889
-12.551386	-2.116391	0.600576	0.002372	0.709897
-12.401180	-2.147426	0.605581	0.002344	0.709888
-13.016731	-2.162684	0.610586	0.002459	0.709638
-13.686102	-2.063070	0.615590	0.002584	0.709599
-13.482051	-2.103661	0.620595	0.002546	0.709590
-12.905381	-2.201215	0.625600	0.002439	0.709600
-13.620373	-2.078484	0.630605	0.002572	0.709590
-13.563448	-2.088055	0.635610	0.002561	0.709591
-13.079624	-2.192749	0.640614	0.002472	0.709554
-14.154171	-2.149545	0.645619	0.002672	0.709257
-14.120792	-2.150668	0.650624	0.002666	0.709266
-14.553774	-2.075891	0.655629	0.002746	0.709261
-14.162909	-2.143651	0.660634	0.002674	0.709265
-14.381360	-2.103480	0.665638	0.002715	0.709267
-14.777974	-2.037447	0.670643	0.002789	0.709257
-14.200000	-2.157549	0.675648	0.002681	0.709223
-15.175692	-2.117071	0.680653	0.002863	0.708956
-15.309880	-2.092269	0.685658	0.002888	0.708957
-15.206995	-2.110226	0.690662	0.002869	0.708957
-15.143760	-2.125366	0.695667	0.002858	0.708949
-15.150011	-2.116972	0.700672	0.002859	0.708964
-15.201391	-2.114219	0.705677	0.002869	0.708951
-14.982328	-2.186566	0.710682	0.002828	0.708884
-16.095122	-2.107708	0.715686	0.003035	0.708644
-16.331083	-2.070184	0.720691	0.003079	0.708635
-16.006693	-2.123061	0.725696	0.003019	0.708644
-16.154031	-2.100708	0.730701	0.003047	0.708636
-16.337542	-2.066492	0.735706	0.003081	0.708639
-16.193975	-2.091389	0.740710	0.003054	0.708640
-16.302263	-2.076113	0.745715	0.003075	0.708632
-16.314379	-2.194862	0.750720	0.003077	0.708389
-17.044978	-2.085146	0.755725	0.003213	0.708348
-16.883961	-2.110660	0.760730	0.003184	0.708354
-16.824314	-2.122548	0.765734	0.003173	0.708351
-17.422531	-2.018274	0.770739	0.003284	0.708346
-16.822039	-2.120754	0.775744	0.003172	0.708355
-16.864416	-2.126884	0.780749	0.003180	0.708327
-17.756403	-2.124030	0.785754	0.003347	0.708014
-17.958199	-2.086087	0.790758	0.003384	0.708018
-18.171066	-2.052634	0.795763	0.003424	0.708008
-17.960105	-2.086585	0.800768	0.003385	0.708015
-18.259405	-2.034807	0.805773	0.003441	0.708012
-17.892358	-2.099576	0.810778	0.003373	0.708013
-17.755112	-2.123543	0.815782	0.003347	0.708014
-18.386664	-2.126247	0.820787	0.003465	0.707782
-19.019193	-2.052121	0.825792	0.003583	0.707705
-19.028009	-2.056514	0.830797	0.003585	0.707692
-18.969336	-2.064375	0.835802	0.003574	0.707697
-18.954799	-2.064991	0.840806	0.003571	0.707701
-19.005972	-2.058877	0.845811	0.003581	0.707695
-18.797376	-2.089997	0.850816	0.003543	0.707706
-18.949586	-2.097665	0.855821	0.003571	0.707636
-19.491266	-2.133125	0.860826	0.003672	0.707371
-19.455157	-2.136926	0.865830	0.003665	0.707376
-20.246561	-1.998673	0.870835	0.003813	0.707370
-19.711269	-2.091179	0.875840	0.003713	0.707376
-19.494142	-2.132730	0.880845	0.003673	0.707370
-19.883702	-2.060308	0.885850	0.003746	0.707375
-19.681921	-2.125028	0.890854	0.003708	0.707317
-20.403928	-2.117900	0.895859	0.003843	0.707073
-20.334047	-2.127917	0.900864	0.003830	0.707078
-20.695331	-2.065278	0.905869	0.003898	0.707074
-20.308417	-2.133555	0.910874	0.003826	0.707075
-20.162637	-2.156401	0.915878	0.003799	0.707081
-20.826591	-2.042066	0.920883	0.003922	0.707073
-20.353658	-2.219790	0.925888	0.003835	0.706885
-21.353953	-2.111062	0.930893	0.004021	0.706745
-21.591730	-2.066434	0.935898	0.004065	0.706749
-21.260914	-2.123275	0.940902	0.004004	0.706753
-21.581175	-2.070628	0.945907	0.004064	0.706744
-21.323102	-2.113493	0.950912	0.004016	0.706750
-21.472642	-2.087779	0.955917	0.004044	0.706748
-21.940747	-2.115702	0.960922	0.004131	0.706524
-22.350432	-2.083121	0.965926	0.004208	0.706442
-22.636740	-2.035279	0.970931	0.004261	0.706435
-21.859634	-2.170045	0.975936	0.004117	0.706443
-21.994022	-2.148158	0.980941	0.004142	0.706438
-22.526584	-2.051837	0.985946	0.004241	0.706441
-22.382319	-2.074922	0.990950	0.004214	0.706446
-22.667134	-2.128244	0.995955	0.004267	0.706236
-23.484239	-2.034625	1.000960	0.004420	0.706131
-23.438354	-2.047241	1.005965	0.004411	0.706122
-23.061267	-2.112606	1.010970	0.004341	0.706125
-22.863426	-2.145476	1.015974	0.004305	0.706130
-23.294956	-2.072871	1.020979	0.004385	0.706121
-22.999394	-2.121841	1.025984	0.004330	0.706128
-23.196468	-2.162652	1.030989	0.004367	0.705975
-24.336871	-2.015687	1.035994	0.004580	0.705862
-23.923540	-2.087632	1.040998	0.004503	0.705865
-24.135874	-2.054525	1.046003	0.004542	0.705855
-23.904960	-2.090459	1.051008	0.004500	0.705865
-24.160247	-2.048764	1.056013	0.004547	0.705857
-24.155511	-2.048725	1.061018	0.004547	0.705859
-23.778700	-2.216834	1.066022	0.004477	0.705655
-25.146133	-2.041274	1.071027	0.004731	0.705518
-24.531598	-2.147034	1.076032	0.004617	0.705525
-24.425406	-2.168457	1.081037	0.004597	0.705520
-24.750493	-2.110475	1.086042	0.004658	0.705520
-24.784343	-2.101425	1.091046	0.004665	0.705526
-24.979881	-2.104860	1.096051	0.004701	0.705448
-25.668737	-2.098829	1.101056	0.004830	0.705213
-25.799844	-2.077598	1.106061	0.004854	0.705208
-25.732306	-2.090152	1.111066	0.004842	0.705207
-25.402371	-2.146808	1.116070	0.004780	0.705211
-26.016364	-2.041276	1.121075	0.004895	0.705203
-25.883477	-2.059276	1.126080	0.004870	0.705214
-25.448815	-2.174690	1.131085	0.004790	0.705137
-26.624279	-2.092046	1.136090	0.005009	0.704881
-26.600244	-2.092077	1.141094	0.005004	0.704890
-26.779416	-2.066074	1.146099	0.005038	0.704877
-26.200770	-2.165057	1.151104	0.004930	0.704886
-26.593615	-2.098287	1.156109	0.005003	0.704879
-26.858695	-2.048636	1.161114	0.005053	0.704883
-26.328270	-2.188894	1.166118	0.004954	0.704791
-27.456885	-2.091950	1.171123	0.005165	0.704581
-27.449422	-2.088874	1.176128	0.005163	0.704589
-27.450258	-2.091136	1.181133	0.005164	0.704584
-27.496021	-2.082173	1.186138	0.005172	0.704585
-27.595712	-2.061388	1.191142	0.005191	0.704591
-27.604010	-2.063947	1.196147	0.005193	0.704583
-27.363269	-2.165168	1.201152	0.005148	0.704465
-28.676001	-2.036078	1.206157	0.005393	0.704253
-28.411436	-2.081087	1.211162	0.005344	0.704257
-28.051869	-2.142839	1.216166	0.005277	0.704262
-28.453575	-2.073206	1.221171	0.005352	0.704257
-28.518905	-2.058703	1.226176	0.005364	0.704263
-28.425307	-2.077412	1.231181	0.005347	0.704258
-28.323254	-2.134369	1.236186	0.005328	0.704180
-29.022519	-2.122150	1.241190	0.005458	0.703953
-29.202849	-2.093762	1.246195	0.005492	0.703945
-29.348843	-2.064299	1.251200	0.005519	0.703952
-29.305453	-2.074250	1.256205	0.005511	0.703947
-29.350538	-2.066143	1.261210	0.005520	0.703947
-29.126285	-2.103000	1.266214	0.005478	0.703953
-29.462860	-2.078641	1.271219	0.005541	0.703881
-29.997548	-2.104647	1.276224	0.005641	0.703635
-29.853850	-2.132597	1.281229	0.005614	0.703630
-30.036956	-2.100617	1.286234	0.005649	0.703629
-30.043839	-2.095918	1.291238	0.005650	0.703636
-30.243844	-2.066379	1.296243	0.005687	0.703623
-30.030142	-2.097643	1.301248	0.005648	0.703636
-29.966789	-2.167390	1.306253	0.005636	0.703518
-31.160177	-2.043061	1.311258	0.005858	0.703339
-30.558974	-2.147633	1.316262	0.005747	0.703344
-30.956096	-2.080858	1.321267	0.005821	0.703336
-30.816946	-2.101269	1.326272	0.005795	0.703344
-30.740410	-2.117979	1.331277	0.005781	0.703338
-30.689252	-2.126027	1.336282	0.005772	0.703340
-31.008192	-2.201221	1.341286	0.005831	0.703073
-32.007712	-2.060117	1.346291	0.006017	0.702998
-31.665620	-2.117256	1.351296	0.005954	0.703005
-31.548925	-2.139618	1.356301	0.005932	0.703002
-32.209360	-2.020983	1.361306	0.006055	0.703003
-31.619712	-2.123575	1.366310	0.005946	0.703008
-31.709410	-2.110567	1.371315	0.005963	0.703002
-32.579972	-2.103329	1.376320	0.006125	0.702703
-33.019625	-2.032209	1.381325	0.006207	0.702688
-33.124086	-2.012742	1.386330	0.006226	0.702689
-32.319397	-2.152096	1.391334	0.006077	0.702697
-32.755260	-2.079411	1.396339	0.006158	0.702687
-32.669051	-2.089538	1.401344	0.006142	0.702697
-32.595267	-2.106025	1.406349	0.006129	0.702690
-33.143775	-2.118840	1.411354	0.006231	0.702466
-33.847162	-2.040575	1.416358	0.006362	0.702370
-33.523564	-2.099982	1.421363	0.006302	0.702367
-33.579848	-2.085708	1.426368	0.006312	0.702375
-33.670408	-2.073392	1.431373	0.006329	0.702367
-33.365300	-2.128190	1.436378	0.006273	0.702366
-33.229240	-2.148096	1.441382	0.006248	0.702374
-33.999419	-2.118823	1.446387	0.006391	0.702155
-34.355442	-2.094831	1.451392	0.006458	0.702075
-34.169737	-2.129651	1.456397	0.006423	0.702072
-34.679098	-2.036867	1.461402	0.006518	0.702075
-34.396661	-2.084922	1.466406	0.006466	0.702080
-34.329168	-2.100439	1.471411	0.006453	0.702072
-34.194611	-2.119539	1.476416	0.006428	0.702082
-34.942240	-2.141570	1.481421	0.006568	0.701767
-35.325019	-2.084703	1.486426	0.006639	0.701744
-35.247119	-2.095516	1.491430	0.006625	0.701750
-35.482962	-2.058022	1.496435	0.006669	0.701740
-35.415692	-2.067789	1.501440	0.006657	0.701745
-35.173958	-2.113140	1.506445	0.006612	0.701740
-35.502863	-2.054230	1.511450	0.006673	0.701740
-35.740372	-2.128392	1.516454	0.006718	0.701504
-36.530530	-2.024515	1.521459	0.006865	0.701429
-36.185617	-2.080784	1.526464	0.006801	0.701439
-36.142382	-2.090199	1.531469	0.006793	0.701435
-36.079387	-2.103484	1.536474	0.006781	0.701431
-35.956863	-2.122102	1.541478	0.006759	0.701437
-36.473811	-2.033284	1.546483	0.006855	0.701430
-36.411841	-2.153972	1.551488	0.006844	0.701208
-36.944884	-2.101706	1.556493	0.006943	0.701121
-36.950156	-2.102393	1.561498	0.006944	0.701117
-36.812090	-2.123862	1.566502	0.006919	0.701123
-37.142367	-2.070023	1.571507	0.006980	0.701113
-36.971853	-2.095544	1.576512	0.006949	0.701122
-37.101395	-2.074417	1.581517	0.006973	0.701118
-37.497627	-2.125173	1.586522	0.007047	0.700872
-37.283728	-2.160359	1.591526	0.007007	0.700877
-37.908882	-2.053471	1.596531	0.007124	0.700868
-37.635823	-2.099168	1.601536	0.007073	0.700874
-37.275240	-2.163940	1.606541	0.007006	0.700872
-37.645248	-2.100355	1.611546	0.007075	0.700867
-37.825104	-2.200933	1.616550	0.007109	0.700598
-38.575584	-2.101609	1.621555	0.007249	0.700528
-38.555507	-2.101193	1.626560	0.007245	0.700536
-38.708561	-2.076449	1.631565	0.007274	0.700530
-38.941005	-2.036122	1.636570	0.007317	0.700528
-38.538690	-2.104333	1.641574	0.007242	0.700534
-38.819734	-2.059536	1.646579	0.007295	0.700523
-39.165910	-2.147049	1.651584	0.007359	0.700220
-39.106642	-2.159243	1.656589	0.007349	0.700217
-39.576621	-2.077208	1.661594	0.007436	0.700213
-39.418423	-2.100233	1.666598	0.007407	0.700223
-39.567597	-2.078142	1.671603	0.007435	0.700214
-39.227339	-2.135173	1.676608	0.007372	0.700221
-39.445338	-2.163339	1.681613	0.007412	0.700085
-40.646117	-2.044767	1.686618	0.007636	0.699890
-39.986994	-2.159359	1.691622	0.007514	0.699896
-40.609864	-2.053903	1.696627	0.007630	0.699884
-40.597763	-2.049914	1.701632	0.007628	0.699897
-40.164697	-2.129462	1.706637	0.007547	0.699892
-40.409623	-2.085945	1.711642	0.007593	0.699891
-40.594994	-2.100319	1.716646	0.007628	0.699794
-41.069587	-2.114900	1.721651	0.007716	0.699593
-40.698102	-2.176930	1.726656	0.007647	0.699601
-41.327218	-2.064587	1.731661	0.007764	0.699601
-41.386813	-2.055967	1.736666	0.007776	0.699597
-40.841139	-2.150599	1.741670	0.007674	0.699602
-41.360202	-2.062882	1.746675	0.007771	0.699592
-41.416537	-2.158405	1.751680	0.007782	0.699377
-42.107185	-2.089546	1.756685	0.007910	0.699266
-42.090267	-2.092072	1.761690	0.007907	0.699267
-41.892052	-2.124164	1.766694	0.007871	0.699273
-42.258698	-2.063125	1.771699	0.007939	0.699264
-41.863894	-2.131623	1.776704	0.007866	0.699268
-41.984703	-2.109202	1.781709	0.007888	0.699269
-42.651904	-2.124232	1.786714	0.008013	0.698997
-42.656999	-2.140118	1.791718	0.008014	0.698962
-42.805191	-2.117999	1.796723	0.008042	0.698953
-43.041404	-2.071346	1.801728	0.008086	0.698962
-42.906645	-2.096771	1.806733	0.008061	0.698959
-42.941334	-2.092858	1.811738	0.008067	0.698954
-43.039811	-2.069926	1.816742	0.008086	0.698965
-43.504569	-2.141885	1.821747	0.008173	0.698650
-43.514348	-2.144296	1.826752	0.008174	0.698641
-43.926159	-2.070203	1.831757	0.008251	0.698642
-44.058797	-2.047822	1.836762	0.008276	0.698639
-43.687507	-2.110365	1.841766	0.008207	0.698646
-43.797805	-2.095231	1.846771	0.008228	0.698637
-43.801243	-2.095931	1.851776	0.008229	0.698634
-44.326454	-2.139608	1.856781	0.008327	0.698354
-44.503084	-2.110300	1.861786	0.008360	0.698350
-44.637201	-2.082435	1.866790	0.008385	0.698357
-44.727108	-2.071703	1.871795	0.008402	0.698346
-44.231806	-2.157365	1.876800	0.008310	0.698351
-44.660224	-2.080348	1.881805	0.008389	0.698352
-44.787548	-2.111025	1.886810	0.008413	0.698243
-45.200850	-2.147959	1.891814	0.008490	0.698018
-45.215747	-2.149491	1.896819	0.008493	0.698009
-45.614372	-2.074142	1.901824	0.008568	0.698017
-45.446956	-2.105468	1.906829	0.008537	0.698014
-45.251884	-2.143146	1.911834	0.008501	0.698008
-45.203211	-2.146695	1.916838	0.008492	0.698018
-45.778289	-2.158955	1.921843	0.008599	0.697784
-46.303667	-2.106280	1.926848	0.008697	0.697700
-46.271454	-2.111267	1.931853	0.008691	0.697702
-46.584748	-2.057464	1.936858	0.008749	0.697697
-46.235505	-2.115931	1.941862	0.008685	0.697705
-46.288053	-2.110706	1.946867	0.008695	0.697696
-46.485417	-2.072636	1.951872	0.008731	0.697701
-46.744516	-2.135679	1.956877	0.008780	0.697479
-47.559503	-2.041980	1.961882	0.008932	0.697373
-47.178791	-2.105564	1.966886	0.008861	0.697382
-47.528286	-2.047410	1.971891	0.008926	0.697373
-47.550871	-2.040093	1.976896	0.008931	0.697379
-47.107264	-2.120453	1.981901	0.008848	0.697376
-47.552967	-2.043414	1.986906	0.008931	0.697371
-47.306228	-2.129084	1.991910	0.008886	0.697286
-48.270537	-2.060293	1.996915	0.009065	0.697075
-48.048669	-2.097168	2.001920	0.009024	0.697081
-48.210128	-2.067311	2.011917	0.009054	0.697082
-48.484519	-2.019725	2.021914	0.009106	0.697079
-47.963808	-2.112506	2.031910	0.009009	0.697078
-47.996536	-2.104729	2.041907	0.009016	0.697082
-48.211463	-2.065104	2.051904	0.009056	0.697084
-48.102333	-2.086004	2.061901	0.009036	0.697080
-48.029725	-2.099393	2.071898	0.009023	0.697079
-48.110459	-2.085239	2.081894	0.009038	0.697078
-47.975680	-2.108490	2.091891	0.009013	0.697079
-48.218955	-2.064039	2.101888	0.009059	0.697080
-47.768070	-2.144595	2.111885	0.008975	0.697079
-48.261414	-2.056881	2.121882	0.009067	0.697078
-48.045397	-2.096310	2.131878	0.009027	0.697076
-48.065721	-2.091128	2.141875	0.009031	0.697078
-47.537831	-2.070840	2.151872	0.008933	0.697311
-47.244926	-2.090296	2.161869	0.008879	0.697377
-47.276692	-2.085452	2.171866	0.008885	0.697375
-47.171872	-2.104165	2.181862	0.008866	0.697374
-47.222082	-2.038625	2.191859	0.008876	0.697489
-46.194673	-2.117457	2.201856	0.008685	0.697701
-46.304658	-2.099161	2.211853	0.008706	0.697698
-46.378007	-2.087170	2.221850	0.008720	0.697695
-46.013799	-2.126426	2.231846	0.008652	0.697747
-45.290163	-2.126453	2.241843	0.008518	0.698009
-45.252102	-2.132298	2.251840	0.008511	0.698010
-45.395690	-2.106204	2.261837	0.008538	0.698010
-45.626084	-2.026566	2.271834	0.008581	0.698088
-44.504918	-2.099118	2.281830	0.008373	0.698347
-44.527634	-2.092547	2.291827	0.008377	0.698351
-44.361520	-2.121346	2.301824	0.008347	0.698352
-44.304088	-2.053937	2.311821	0.008336	0.698510
-43.955098	-2.052889	2.321818	0.008272	0.698638
-43.747257	-2.090821	2.331814	0.008233	0.698635
-43.756735	-2.064697	2.341811	0.008235	0.698685
-42.636555	-2.129066	2.351808	0.008027	0.698959
-42.661843	-2.125958	2.361805	0.008032	0.698956
-43.053607	-2.056027	2.371802	0.008105	0.698955
-42.641383	-2.055633	2.381798	0.008029	0.699105
-41.964579	-2.096214	2.391795	0.007903	0.699267
-41.817875	-2.121857	2.401792	0.007876	0.699267
-42.027044	-2.084339	2.411789	0.007915	0.699267
-41.180471	-2.077035	2.421786	0.007758	0.699588
-40.897778	-2.122155	2.431782	0.007706	0.699598
-41.108959	-2.083125	2.441779	0.007745	0.699600
-40.782004	-2.093364	2.451776	0.007685	0.699697
-40.248694	-2.089252	2.461773	0.007586	0.699898
-40.375136	-2.068030	2.471770	0.007609	0.699895
-40.145076	-2.109845	2.481766	0.007567	0.699893
-39.737120	-2.036998	2.491763	0.007491	0.700187
-39.436981	-2.073394	2.501760	0.007436	0.700222
-39.347045	-2.089026	2.511757	0.007419	0.700222
-39.063646	-2.056571	2.521754	0.007367	0.700390
-38.480007	-2.089086	2.531750	0.007258	0.700534
-38.641286	-2.059996	2.541747	0.007289	0.700534
-38.380149	-2.090313	2.551744	0.007240	0.700567
-37.874472	-2.028649	2.561741	0.007147	0.700874
-37.522754	-2.091348	2.571738	0.007081	0.700873
-37.712750	-2.056752	2.581734	0.007117	0.700874
-37.352730	-2.044668	2.591731	0.007050	0.701028
-36.937170	-2.071796	2.601728	0.006973	0.701122
-36.997814	-2.060614	2.611725	0.006985	0.701123
-36.790904	-2.034744	2.621722	0.006947	0.701249
-36.170633	-2.053659	2.631718	0.006831	0.701434
-36.001306	-2.083524	2.641715	0.006800	0.701434
-35.847771	-2.098065	2.651712	0.006772	0.701460
-35.234721	-2.068238	2.661709	0.006658	0.701741
-35.030630	-2.104688	2.671706	0.006620	0.701740
-35.209700	-2.073045	2.681702	0.006654	0.701739
-34.734777	-2.061839	2.691699	0.006566	0.701932
-33.976205	-2.127845	2.701696	0.006425	0.702072
-34.129379	-2.100512	2.711693	0.006454	0.702071
-34.184773	-2.090305	2.721690	0.006464	0.702071
-33.670249	-2.046452	2.731686	0.006369	0.702345
-33.226992	-2.111860	2.741683	0.006287	0.702372
-33.273351	-2.103960	2.751680	0.006296	0.702371
-33.221172	-2.038279	2.761677	0.006286	0.702522
-32.418627	-2.097208	2.771674	0.006137	0.702691
-32.588183	-2.067690	2.781670	0.006169	0.702689
-32.562389	-2.055871	2.791667	0.006164	0.702722
-31.737062	-2.061998	2.801664	0.006011	0.703006
-31.523951	-2.100053	2.811661	0.005972	0.703005
-31.521557	-2.100034	2.821658	0.005972	0.703006
-31.252483	-2.053137	2.831654	0.005922	0.703197
-30.624801	-2.093689	2.841651	0.005805	0.703340
-30.748825	-2.070086	2.851648	0.005829	0.703342
-30.773215	-2.057471	2.861645	0.005833	0.703359
-29.904161	-2.077335	2.871642	0.005672	0.703631
-29.905933	-2.076573	2.881638	0.005673	0.703631
-29.825126	-2.090186	2.891635	0.005658	0.703632
-29.417911	-2.065814	2.901632	0.005582	0.703827
-28.830115	-2.109335	2.911629	0.005473	0.703950
-29.048089	-2.070493	2.921626	0.005514	0.703949
-29.033024	-2.062193	2.931622	0.005512	0.703971
-28.057111	-2.093264	2.941619	0.005330	0.704258
-28.091832	-2.086551	2.951616	0.005337	0.704259
-28.124251	-2.080674	2.961613	0.005343	0.704259
-27.621663	-2.076352	2.971610	0.005250	0.704447
-27.285113	-2.067148	2.981606	0.005188	0.704586
-27.223385	-2.077358	2.991603	0.005176	0.704587
-27.396499	-2.026385	3.001600	0.005209	0.704627
-26.324564	-2.089678	3.011597	0.005010	0.704884
-26.220327	-2.108474	3.021594	0.004991	0.704883
-26.454277	-2.065816	3.031590	0.005034	0.704884
-25.905005	-2.072870	3.041587	0.004932	0.705067
-25.690839	-2.038560	3.051584	0.004893	0.705212
-25.312984	-2.105087	3.061581	0.004823	0.705213
-25.363142	-2.088245	3.071578	0.004832	0.705228
-24.747463	-2.050388	3.081574	0.004718	0.705525
-24.526257	-2.087395	3.091571	0.004677	0.705529
-24.690398	-2.057766	3.101568	0.004708	0.705529
-24.149846	-2.048294	3.111565	0.004608	0.705742
-23.726457	-2.061349	3.121562	0.004529	0.705867
-23.560269	-2.092549	3.131558	0.004499	0.705863
-23.397529	-2.121657	3.141555	0.004469	0.705862
-23.188990	-2.034792	3.151552	0.004430	0.706111
-22.906425	-2.076048	3.161549	0.004378	0.706129
-23.169389	-2.030086	3.171546	0.004427	0.706126
-22.392381	-2.052479	3.181542	0.004283	0.706359
-22.186395	-2.046634	3.191539	0.004245	0.706444
-22.131416	-2.053927	3.201536	0.004235	0.706449
-21.875680	-2.040062	3.211533	0.004187	0.706567
-21.388667	-2.034574	3.221530	0.004097	0.706752
-21.027584	-2.099387	3.231526	0.004030	0.706751
-21.423907	-2.019579	3.241523	0.004104	0.706769
-20.339899	-2.056562	3.251520	0.003903	0.707082
-20.134757	-2.093499	3.261517	0.003865	0.707080
-20.464035	-2.033347	3.271514	0.003926	0.707083
-20.194729	-2.004985	3.281510	0.003876	0.707235
-19.477077	-2.062011	3.291507	0.003743	0.707377
-19.559158	-2.045298	3.301504	0.003759	0.707381
-19.407058	-2.047932	3.311501	0.003731	0.707429
-18.661216	-2.044234	3.321498	0.003592	0.707703
-18.395943	-2.092745	3.331494	0.003543	0.707700
-18.490220	-2.075573	3.341491	0.003561	0.707700
-18.067310	-2.075335	3.351488	0.003483	0.707851
-17.598276	-2.076439	3.361485	0.003395	0.708016
-17.689416	-2.060878	3.371482	0.003413	0.708014
-17.579001	-2.080735	3.381478	0.003392	0.708013
-16.833796	-2.055037	3.391475	0.003254	0.708330
-16.532205	-2.098009	3.401472	0.003198	0.708351
-16.560662	-2.092295	3.411469	0.003204	0.708352
-16.613104	-2.064599	3.421466	0.003214	0.708388
-16.086376	-2.033859	3.431462	0.003116	0.708637
-15.914218	-2.062184	3.441459	0.003084	0.708641
-15.723050	-2.095653	3.451456	0.003049	0.708642
-15.424593	-2.024179	3.461453	0.002994	0.708891
-15.321521	-2.008064	3.471450	0.002975	0.708959
-14.966909	-2.073394	3.481446	0.002909	0.708954
-14.948819	-2.005625	3.491443	0.002906	0.709096
-14.068669	-2.077029	3.501440	0.002743	0.709266
-14.215132	-2.050206	3.511437	0.002770	0.709267
-14.131666	-2.065611	3.521434	0.002755	0.709266
-13.467181	-2.020964	3.531430	0.002631	0.709591
-13.082198	-2.085728	3.541427	0.002560	0.709598
-13.088252	-2.084046	3.551424	0.002561	0.709599
-13.085147	-2.024715	3.561421	0.002561	0.709718
-12.301977	-2.076210	3.571418	0.002416	0.709894
-12.211614	-2.092883	3.581414	0.002399	0.709892
-12.290803	-2.078324	3.591411	0.002414	0.709892
-11.647547	-2.073694	3.601408	0.002295	0.710130
-11.097692	-2.125442	3.611405	0.002193	0.710222
-11.231696	-2.102287	3.621402	0.002218	0.710220
-11.163249	-2.114390	3.631398	0.002205	0.710220
-10.387811	-2.127621	3.641395	0.002061	0.710469
-9.986323	-2.165464	3.651392	0.001987	0.710535
-10.279750	-2.113470	3.661389	0.002042	0.710534
-10.013827	-2.161038	3.671386	0.001993	0.710533
-9.676846	-2.095330	3.681382	0.001930	0.710784
-9.261078	-2.124778	3.691379	0.001853	0.710872
-8.994743	-2.171949	3.701376	0.001804	0.710872
-9.210965	-2.131601	3.711373	0.001844	0.710875
-8.849045	-2.084332	3.721370	0.001777	0.711098
-8.562696	-2.113920	3.731366	0.001724	0.711140
-8.345983	-2.150368	3.741363	0.001684	0.711144
-8.313663	-2.094971	3.751360	0.001679	0.711265
-7.536221	-2.136608	3.761357	0.001534	0.711458
-7.561188	-2.133240	3.771354	0.001539	0.711455
-7.532014	-2.137913	3.781350	0.001534	0.711456
-6.773677	-2.160126	3.791347	0.001393	0.711680
-6.516481	-2.161764	3.801344	0.001345	0.711768
-6.703864	-2.128240	3.811341	0.001381	0.711768
-6.432607	-2.177030	3.821338	0.001330	0.711766
-5.825037	-2.124009	3.831334	0.001218	0.712087
-5.627301	-2.155462	3.841331	0.001181	0.712094
-5.677188	-2.145537	3.851328	0.001191	0.712095
-5.541124	-2.122582	3.861325	0.001166	0.712189
-4.842313	-2.147675	3.871322	0.001036	0.712386
-4.942021	-2.129108	3.881318	0.001055	0.712387
-4.606758	-2.187653	3.891315	0.000993	0.712389
-4.238969	-2.124296	3.901312	0.000924	0.712645
-3.917645	-2.147463	3.911309	0.000865	0.712713
-3.993170	-2.132420	3.921306	0.000879	0.712715
-3.972801	-2.093008	3.931302	0.000876	0.712800
-3.036811	-2.146049	3.941299	0.000702	0.713026
-3.136703	-2.125487	3.951296	0.000721	0.713031
-2.989243	-2.152648	3.961293	0.000694	0.713029
-2.639150	-2.078471	3.971290	0.000629	0.713300
-2.340296	-2.101685	3.981286	0.000573	0.713359
-2.212255	-2.122125	3.991283	0.000550	0.713363
-2.112512	-2.082825	4.001280	0.000531	0.713476
-1.685843	-2.070750	4.011277	0.000452	0.713650
-1.751806	-2.057882	4.021274	0.000465	0.713652
-1.515798	-2.056005	4.031270	0.000421	0.713739
-1.407464	-1.958315	4.041267	0.000401	0.713971
-1.342195	-1.968867	4.051264	0.000389	0.713972
-1.374493	-1.868506	4.061261	0.000396	0.714160
-1.210652	-1.838278	4.071258	0.000366	0.714277
-1.133747	-1.803096	4.081254	0.000351	0.714374
-0.989334	-1.709210	4.091251	0.000325	0.714611
-0.855315	-1.705753	4.101248	0.000300	0.714664
-0.948857	-1.564147	4.111245	0.000318	0.714912
-1.088623	-1.488629	4.121242	0.000344	0.715012
-1.045968	-1.384898	4.131238	0.000336	0.715232
-0.930886	-1.300655	4.141235	0.000315	0.715439
-0.735208	-1.267949	4.151232	0.000279	0.715573
-0.742763	-1.106529	4.161229	0.000281	0.715889
-0.632856	-1.056567	4.171226	0.000260	0.716027
-0.841133	-0.939971	4.181222	0.000299	0.716183
-0.783347	-0.815273	4.191219	0.000289	0.716450
-0.543299	-0.726937	4.201216	0.000244	0.716709
-0.549291	-0.608114	4.211213	0.000246	0.716942
-0.390046	-0.515487	4.221210	0.000216	0.717181
-0.330388	-0.406186	4.231206	0.000206	0.717417
-0.415955	-0.245954	4.241203	0.000222	0.717703
-0.435699	-0.086514	4.251200	0.000226	0.718011
-0.320060	0.045517	4.261197	0.000204	0.718312
0.000000	0.137350	4.271194	0.000145	0.718605
-0.160169	0.802645	4.276198	0.000174	0.719861
-0.096431	2.034999	4.281203	0.000162	0.722308
0.218818	3.830371	4.286208	0.000102	0.725935
0.434311	6.199960	4.291213	0.000061	0.730626
0.530934	9.086817	4.296218	0.000041	0.736243
0.930003	12.406053	4.301222	-0.000035	0.742747
1.448970	16.152297	4.306227	-0.000134	0.750043
1.648551	20.369879	4.311232	-0.000174	0.758045
2.078384	24.938080	4.316237	-0.000257	0.766688
2.566758	29.864033	4.321242	-0.000351	0.775907
3.007961	35.149012	4.326246	-0.000436	0.785652
3.149150	40.805482	4.331251	-0.000466	0.795845
3.760623	46.669259	4.336256	-0.000584	0.806420
4.400812	52.828850	4.341261	-0.000707	0.817380
5.176549	59.227787	4.346266	-0.000855	0.828646
5.999164	65.871188	4.351270	-0.001013	0.840187
6.528038	72.773230	4.356275	-0.001115	0.851916
7.027882	79.885380	4.361280	-0.001213	0.863822
7.478910	87.209933	4.366285	-0.001302	0.875895
7.985246	94.675340	4.371290	-0.001401	0.888045
10.896971	101.908494	4.376294	-0.001947	0.900330
13.267055	109.425991	4.381299	-0.002393	0.912743
14.046685	117.350154	4.386304	-0.002544	0.925183
14.733829	125.415528	4.391309	-0.002677	0.937647
15.358235	133.589196	4.396314	-0.002798	0.950093
16.175229	141.808409	4.401318	-0.002955	0.962494
17.115285	150.099375	4.406323	-0.003136	0.974872
17.860240	158.494789	4.411328	-0.003280	0.987195
19.033940	166.886483	4.416333	-0.003504	0.999467
19.659684	175.386898	4.421338	-0.003625	1.011608
21.103629	183.806171	4.426342	-0.003900	1.023689
22.009783	192.364940	4.431347	-0.004074	1.035692
22.842795	200.955328	4.436352	-0.004234	1.047582
24.123534	209.520295	4.441357	-0.004478	1.059408
24.765476	218.204294	4.446362	-0.004603	1.071115
25.660085	226.853419	4.451366	-0.004775	1.082705
26.493131	235.519147	4.456371	-0.004936	1.094180
27.446100	244.152366	4.461376	-0.005119	1.105521
28.345517	252.812445	4.466381	-0.005292	1.116768
29.364163	261.425739	4.471386	-0.005487	1.127869
30.377093	270.066504	4.476390	-0.005681	1.138895
31.034831	278.770410	4.481395	-0.005809	1.149817
31.998775	287.409888	4.486400	-0.005994	1.160621
32.921669	296.034281	4.491405	-0.006171	1.171299
33.417804	304.700325	4.496410	-0.006269	1.181842
34.276126	313.310803	4.501414	-0.006434	1.192299
35.234288	321.871279	4.506419	-0.006618	1.202625
35.881855	330.489743	4.511424	-0.006744	1.212870
36.325857	339.133044	4.516429	-0.006832	1.223017
36.860281	347.746597	4.521434	-0.006937	1.233063
37.540042	356.297121	4.526438	-0.007069	1.242985
38.060489	364.865895	4.531443	-0.007172	1.252817
38.795275	373.373730	4.536448	-0.007314	1.262545
39.679581	381.872978	4.541453	-0.007484	1.272217
40.442559	390.346466	4.546458	-0.007631	1.281764
41.001802	398.865771	4.551462	-0.007741	1.291253
41.430338	407.371977	4.556467	-0.007826	1.300635
42.230342	415.863811	4.561472	-0.007981	1.310000
42.616702	424.434722	4.566477	-0.008058	1.319310
43.231249	432.828777	4.571482	-0.008178	1.328406
43.962136	441.237854	4.576486	-0.008319	1.337477
44.463594	449.640629	4.581491	-0.008418	1.346439
44.954488	458.069439	4.586496	-0.008515	1.355367
45.926535	466.390505	4.591501	-0.008701	1.364207
46.405677	474.800189	4.596506	-0.008795	1.372997
46.980456	483.173360	4.601510	-0.008908	1.381710
47.759571	491.516945	4.606515	-0.009058	1.390373
48.296365	499.886658	4.611520	-0.009163	1.398967
48.805875	508.248433	4.616525	-0.009263	1.407496
49.280504	516.607010	4.621530	-0.009357	1.415965
49.669318	524.966875	4.626534	-0.009435	1.424370
50.242117	533.305204	4.631539	-0.009547	1.432734
50.860762	541.592403	4.636544	-0.009667	1.441007
51.401748	549.927380	4.641549	-0.009773	1.449266
51.971514	558.237597	4.646554	-0.009885	1.457459
52.420426	566.551014	4.651558	-0.009973	1.465590
53.093715	574.874478	4.656563	-0.010104	1.473720
53.761728	583.123145	4.661568	-0.010234	1.481734
54.133076	591.431165	4.666573	-0.010308	1.489715
54.264244	599.756228	4.671578	-0.010338	1.497631
54.833608	608.006292	4.676582	-0.010449	1.505503
55.473194	616.265708	4.681587	-0.010573	1.513353
55.856246	624.522334	4.686592	-0.010650	1.521121
56.682405	632.736514	4.691597	-0.010809	1.528877
57.112929	641.006794	4.696602	-0.010894	1.536585
57.413600	649.290755	4.701606	-0.010956	1.544249
58.076566	657.522544	4.706611	-0.011084	1.551880
58.761834	665.730937	4.711616	-0.011217	1.559456
59.271081	673.969553	4.716621	-0.011317	1.566996
59.486140	682.246562	4.721626	-0.011362	1.574492
60.052854	690.455910	4.726630	-0.011473	1.581943
60.597350	698.671306	4.731635	-0.011580	1.589360
60.948722	706.926917	4.736640	-0.011650	1.596751
61.418687	715.135729	4.741645	-0.011743	1.604083
61.781095	723.365144	4.746650	-0.011816	1.611385
62.145521	731.605453	4.751654	-0.011889	1.618664
62.545107	739.804228	4.756659	-0.011968	1.625878
63.161503	748.043423	4.761664	-0.012088	1.633126
63.646189	756.239750	4.766669	-0.012184	1.640286
64.024130	764.418507	4.771674	-0.012259	1.647385
64.590826	772.611339	4.776678	-0.012370	1.654491
65.020707	780.793148	4.781683	-0.012455	1.661539
65.462674	788.981073	4.786688	-0.012543	1.668564
65.943592	797.178271	4.791693	-0.012637	1.675572
66.070760	805.389249	4.796698	-0.012666	1.682515
66.628178	813.548744	4.801702	-0.012775	1.689444
66.901875	821.756540	4.806707	-0.012831	1.696346
67.408817	829.905345	4.811712	-0.012931	1.703203
67.845049	838.099832	4.816717	-0.013017	1.710060
68.137001	846.294218	4.821722	-0.013077	1.716871
68.492806	854.468699	4.826726	-0.013148	1.723647
68.869836	862.622446	4.831731	-0.013224	1.730382
69.283664	870.795719	4.836736	-0.013306	1.737111
69.694935	878.953105	4.841741	-0.013388	1.743801
70.208162	887.090237	4.846746	-0.013488	1.750462
70.865112	895.238975	4.851750	-0.013616	1.757125
70.930313	903.434877	4.856755	-0.013633	1.763726
71.289538	911.592931	4.861760	-0.013705	1.770309
71.761092	919.761515	4.866765	-0.013798	1.776890
72.170875	927.891056	4.871770	-0.013880	1.783407
72.569922	936.071772	4.876774	-0.013959	1.789940
73.141136	944.237685	4.881779	-0.014071	1.796459
73.494776	952.354446	4.886784	-0.014142	1.802888
73.794537	960.518258	4.891789	-0.014203	1.809325
74.134173	968.663067	4.896794	-0.014271	1.815729
74.438910	976.805207	4.901798	-0.014333	1.822104
75.219691	984.892762	4.906803	-0.014484	1.828472
75.579714	993.058635	4.911808	-0.014556	1.834827
75.894746	1001.214027	4.916813	-0.014620	1.841147
76.274165	1009.338186	4.921818	-0.014695	1.847429
76.538091	1017.525244	4.926822	-0.014750	1.853724
77.108192	1025.623819	4.931827	-0.014861	1.859966
77.455611	1033.757032	4.936832	-0.014931	1.866187
77.805215	1041.939278	4.941837	-0.015001	1.872425
78.075800	1050.072765	4.946842	-0.015057	1.878597
78.393092	1058.194155	4.951846	-0.015121	1.884744
78.678142	1066.322882	4.956851	-0.015179	1.890873
79.121450	1074.428919	4.961856	-0.015267	1.896983
80.044465	1082.476155	4.966861	-0.015444	1.903084
80.306633	1090.622803	4.971866	-0.015498	1.909164
80.611635	1098.780751	4.976870	-0.015560	1.915238
81.073740	1106.884805	4.981875	-0.015651	1.921271
81.723853	1114.954724	4.986880	-0.015777	1.927280
82.089372	1123.115052	4.991885	-0.015850	1.933306
82.516786	1131.235411	4.996890	-0.015935	1.939290
82.723669	1139.376426	5.001894	-0.015979	1.945246
83.141763	1147.524876	5.006899	-0.016062	1.951213
83.899629	1155.604554	5.011904	-0.016208	1.957148
84.609999	1163.666750	5.016909	-0.016345	1.963048
84.827925	1171.794450	5.021914	-0.016391	1.968923
85.209263	1179.933559	5.026918	-0.016467	1.974807
85.893250	1187.981170	5.031923	-0.016599	1.980640
86.522819	1196.063393	5.036928	-0.016722	1.986475
87.121932	1204.188956	5.041933	-0.016839	1.992320
87.492945	1212.311965	5.046938	-0.016913	1.998122
88.206287	1220.389572	5.051942	-0.017051	2.003911
88.301206	1228.554606	5.056947	-0.017074	2.009680
88.489033	1236.705897	5.061952	-0.017114	2.015432
89.024602	1244.803420	5.066957	-0.017218	2.021167
89.185448	1252.925813	5.071962	-0.017254	2.026863
89.538388	1261.057249	5.076966	-0.017324	2.032570
90.051984	1269.146842	5.081971	-0.017425	2.038248
90.450714	1277.217698	5.086976	-0.017505	2.043885
90.913246	1285.316052	5.091981	-0.017596	2.049533
91.383482	1293.398829	5.096986	-0.017688	2.055154
91.622825	1301.519058	5.101990	-0.017738	2.060763
92.262904	1309.577978	5.106995	-0.017862	2.066355
92.526235	1317.700988	5.112000	-0.017917	2.071937
93.044873	1325.804105	5.117005	-0.018018	2.077516
93.523741	1333.851590	5.122010	-0.018113	2.083039
93.830553	1341.990063	5.127014	-0.018175	2.088591
94.227512	1350.099022	5.132019	-0.018254	2.094117
94.592249	1358.186924	5.137024	-0.018327	2.099612
94.899014	1366.299830	5.142029	-0.018389	2.105103
95.198568	1374.410538	5.147034	-0.018450	2.110577
95.667671	1382.547482	5.152038	-0.018543	2.116072
96.106276	1390.595684	5.157043	-0.018629	2.121489
96.396232	1398.673545	5.162048	-0.018688	2.126899
97.152989	1406.727663	5.167053	-0.018834	2.132323
97.529932	1414.804837	5.172058	-0.018910	2.137713
97.816617	1422.900511	5.177062	-0.018968	2.143092
98.474163	1430.949901	5.182067	-0.019096	2.148463
98.747292	1439.078721	5.187072	-0.019152	2.153836
99.305917	1447.149654	5.192077	-0.019261	2.159184
99.589255	1455.232297	5.197082	-0.019319	2.164501
99.979505	1463.332501	5.202086	-0.019397	2.169826
100.412728	1471.432641	5.207091	-0.019482	2.175142
100.482917	1479.537383	5.212096	-0.019501	2.180414
101.181335	1487.591756	5.217101	-0.019636	2.185699
101.606041	1495.686791	5.222106	-0.019720	2.190972
101.883904	1503.814186	5.227110	-0.019777	2.196240
102.315099	1511.870437	5.232115	-0.019862	2.201463
102.859393	1519.904149	5.237120	-0.019969	2.206670
103.176114	1528.035175	5.242125	-0.020033	2.211906
103.320376	1536.131449	5.247130	-0.020065	2.217092
103.819542	1544.174884	5.252134	-0.020163	2.222263
104.551627	1552.206236	5.257139	-0.020304	2.227436
104.891675	1560.319589	5.262144	-0.020373	2.232614
105.183685	1568.415053	5.267149	-0.020432	2.237764
105.528169	1576.466133	5.272154	-0.020501	2.242878
105.598916	1584.572292	5.277158	-0.020520	2.247992
106.182908	1592.643140	5.282163	-0.020634	2.253117
106.476057	1600.727397	5.287168	-0.020693	2.258213
106.869445	1608.816463	5.292173	-0.020772	2.263309
107.312827	1616.865810	5.297178	-0.020859	2.268373
107.725814	1625.026982	5.302182	-0.020941	2.273493
108.134565	1633.073437	5.307187	-0.021023	2.278530
108.232908	1641.143315	5.312192	-0.021046	2.283543
108.642673	1649.201447	5.317197	-0.021127	2.288565
108.952802	1657.273580	5.322202	-0.021190	2.293575
109.323639	1665.338505	5.327206	-0.021264	2.298576
109.930429	1673.360900	5.332211	-0.021382	2.303559
109.988897	1681.464818	5.337216	-0.021398	2.308535
110.416219	1689.549812	5.342221	-0.021483	2.313520
110.686759	1697.602605	5.347226	-0.021539	2.318461
111.010674	1705.663692	5.352230	-0.021604	2.323401
111.374048	1713.742442	5.357235	-0.021677	2.328345
111.695690	1721.809543	5.362240	-0.021742	2.333267
111.886026	1729.912018	5.367245	-0.021782	2.338190
112.345360	1737.948910	5.372250	-0.021873	2.343084
112.806271	1746.003234	5.377254	-0.021964	2.347979
113.112619	1754.130404	5.382259	-0.022026	2.352895
113.212186	1762.196836	5.387264	-0.022050	2.357748
113.743417	1770.227442	5.392269	-0.022154	2.362603
113.881118	1778.302889	5.397274	-0.022184	2.367444
114.448547	1786.352586	5.402278	-0.022295	2.372294
114.721534	1794.445331	5.407283	-0.022351	2.377136
114.876000	1802.511789	5.412288	-0.022385	2.381943
115.180764	1810.580576	5.417293	-0.022447	2.386754
115.525736	1818.658629	5.422298	-0.022516	2.391564
115.629523	1826.743086	5.427302	-0.022541	2.396348
115.991302	1834.779950	5.432307	-0.022613	2.401116
116.137124	1842.840292	5.437312	-0.022645	2.405870
116.508473	1850.898929	5.442317	-0.022720	2.410632
116.671398	1858.996101	5.447322	-0.022755	2.415391
116.972201	1867.038455	5.452326	-0.022816	2.420119
117.361754	1875.072145	5.457331	-0.022894	2.424839
117.445236	1883.160879	5.462336	-0.022914	2.429559
117.860167	1891.305476	5.467341	-0.022997	2.434327
118.208764	1899.300356	5.472346	-0.023067	2.438994
118.685969	1907.332423	5.477350	-0.023161	2.443684
119.005634	1915.386081	5.482355	-0.023225	2.448365
119.172751	1923.449664	5.487360	-0.023262	2.453031
119.412099	1931.527390	5.492365	-0.023311	2.457701
119.540158	1939.576502	5.497370	-0.023340	2.462338
119.866570	1947.635385	5.502374	-0.023406	2.466987
120.265242	1955.706262	5.507379	-0.023485	2.471639
120.499443	1963.759367	5.512384	-0.023534	2.476260
120.664312	1971.823273	5.517389	-0.023570	2.480873
120.896483	1979.863109	5.522394	-0.023618	2.485469
121.290185	1987.912702	5.527398	-0.023697	2.490074
121.563221	1996.006296	5.532403	-0.023753	2.494686
121.885401	2004.030072	5.537408	-0.023818	2.499254
122.465460	2012.058665	5.542413	-0.023931	2.503835
122.661938	2020.139316	5.547418	-0.023972	2.508409
122.965235	2028.239687	5.552422	-0.024034	2.512993
123.105491	2036.312916	5.557427	-0.024065	2.517542
123.271785	2044.349337	5.562432	-0.024101	2.522064
123.877977	2052.359279	5.567437	-0.024219	2.526594
123.865789	2060.461127	5.572442	-0.024222	2.531124
123.964530	2068.546526	5.577446	-0.024246	2.535644
124.467799	2076.557261	5.582451	-0.024344	2.540143
124.777254	2084.578825	5.587456	-0.024407	2.544626
125.059577	2092.657581	5.592461	-0.024465	2.549132
125.435515	2100.715249	5.597466	-0.024540	2.553624
125.678348	2108.777952	5.602470	-0.024590	2.558101
126.012948	2116.823523	5.607475	-0.024658	2.562568
126.201056	2124.870115	5.612480	-0.024698	2.567017
126.358222	2132.962230	5.617485	-0.024732	2.571481
126.657243	2141.015667	5.622490	-0.024793	2.575926
126.923459	2149.063117	5.627494	-0.024848	2.580358
127.239997	2157.100561	5.632499	-0.024912	2.584780
127.453134	2165.155786	5.637504	-0.024956	2.589198
127.962006	2173.380887	5.642509	-0.025056	2.593720
128.310421	2181.394027	5.647514	-0.025126	2.598108
128.542701	2189.395486	5.652518	-0.025175	2.602475
129.047879	2197.377106	5.657523	-0.025274	2.606841
129.292250	2205.397078	5.662528	-0.025324	2.611204
129.534307	2213.497902	5.667533	-0.025374	2.615603
129.772914	2221.510544	5.672538	-0.025424	2.619946
130.307967	2229.500800	5.677542	-0.025529	2.624290
130.429146	2237.597865	5.682547	-0.025556	2.628657
130.409392	2245.690692	5.687552	-0.025558	2.633004
130.781392	2253.724450	5.692557	-0.025632	2.637339
130.781340	2261.760842	5.697562	-0.025637	2.641643
131.109390	2269.791668	5.702566	-0.025703	2.645960
131.580344	2277.820917	5.707571	-0.025796	2.650277
131.710011	2285.899178	5.712576	-0.025825	2.654591
132.082858	2293.953010	5.717581	-0.025900	2.658901
132.077652	2302.009820	5.722586	-0.025904	2.663181
132.339599	2310.049397	5.727590	-0.025958	2.667462
132.766470	2318.098509	5.732595	-0.026042	2.671752
133.014395	2326.154776	5.737600	-0.026094	2.676027
133.209435	2334.215694	5.742605	-0.026135	2.680295
133.414286	2342.213101	5.747610	-0.026178	2.684523
133.632214	2350.280447	5.752614	-0.026224	2.688781
134.086815	2358.341077	5.757619	-0.026314	2.693045
134.420558	2366.350684	5.762624	-0.026381	2.697267
134.690478	2374.406375	5.767629	-0.026436	2.701503
134.828787	2382.448253	5.772634	-0.026467	2.705716
135.203589	2390.478587	5.777638	-0.026542	2.709932
135.583101	2398.559450	5.782643	-0.026618	2.714167
135.835749	2406.587275	5.787648	-0.026670	2.718361
136.012728	2414.636077	5.792653	-0.026708	2.722554
136.364273	2422.668171	5.797658	-0.026779	2.726743
136.410002	2430.749797	5.802662	-0.026792	2.730932
136.662767	2438.826535	5.807667	-0.026844	2.735125
136.980492	2446.831887	5.812672	-0.026909	2.739278
137.199275	2454.879465	5.817677	-0.026954	2.743441
137.333308	2462.934240	5.822682	-0.026984	2.747596
137.802646	2470.990917	5.827686	-0.027077	2.751766
138.209052	2479.086372	5.832691	-0.027158	2.755946
138.268413	2487.105302	5.837696	-0.027174	2.760059
138.599334	2495.112911	5.842701	-0.027241	2.764177
138.713951	2503.161057	5.847706	-0.027267	2.768296
139.010989	2511.204822	5.852710	-0.027327	2.772418
139.224996	2519.284535	5.857715	-0.027372	2.776546
139.381865	2527.300762	5.862720	-0.027407	2.780633
139.780990	2535.312985	5.867725	-0.027486	2.784727
139.749483	2543.387880	5.872730	-0.027485	2.788820
140.149748	2551.430098	5.877734	-0.027565	2.792917
140.365738	2559.478510	5.882739	-0.027610	2.796999
140.508995	2567.510095	5.887744	-0.027642	2.801063
140.675414	2575.544561	5.892749	-0.027678	2.805124
140.916117	2583.572283	5.897754	-0.027728	2.809180
141.272095	2591.617753	5.902758	-0.027799	2.813245
141.482316	2599.667533	5.907763	-0.027844	2.817299
141.737340	2607.690240	5.912768	-0.027896	2.821335
142.007968	2615.734658	5.917773	-0.027952	2.825377
141.892071	2623.811160	5.922778	-0.027935	2.829408
142.589405	2631.840175	5.927782	-0.028070	2.833455
142.898267	2639.892699	5.932787	-0.028133	2.837486
142.703050	2647.948233	5.937792	-0.028101	2.841485
143.211432	2655.946498	5.942797	-0.028201	2.845489
143.277751	2663.983725	5.947802	-0.028219	2.849481
143.373638	2672.057291	5.952806	-0.028242	2.853488
143.775016	2680.099577	5.957811	-0.028321	2.857491
144.015913	2688.120247	5.962816	-0.028371	2.861468
144.223051	2696.152848	5.967821	-0.028415	2.865444
144.254458	2704.213288	5.972826	-0.028426	2.869419
144.847747	2712.234640	5.977830	-0.028541	2.873399
145.283205	2720.274302	5.982835	-0.028628	2.877374
145.440589	2728.288914	5.987840	-0.028662	2.881317
145.757665	2736.337583	5.992845	-0.028726	2.885279
146.053593	2744.369211	5.997850	-0.028786	2.889226
146.303614	2752.440102	6.002854	-0.028838	2.893184
146.464686	2760.494292	6.007859	-0.028873	2.897124
146.580828	2768.529264	6.012864	-0.028900	2.901047
147.018282	2776.537741	6.017869	-0.028986	2.904969
147.092179	2784.614107	6.022874	-0.029005	2.908899
147.442443	2792.694170	6.027878	-0.029075	2.912840
147.733960	2800.762190	6.032883	-0.029135	2.916767
147.943889	2808.749536	6.037888	-0.029179	2.920645
148.243045	2816.734612	6.042893	-0.029240	2.924522
148.631735	2824.764007	6.047898	-0.029317	2.928419
148.804636	2832.814267	6.052902	-0.029355	2.932310
148.821145	2840.917012	6.057907	-0.029363	2.936213
149.002269	2848.897021	6.062912	-0.029401	2.940060
149.422731	2856.939651	6.067917	-0.029485	2.943945
149.476461	2864.984687	6.072922	-0.029500	2.947806
149.627657	2873.038242	6.077926	-0.029533	2.951672
149.938763	2881.104763	6.082931	-0.029596	2.955547
150.020175	2889.107414	6.087936	-0.029616	2.959375
150.294336	2897.126578	6.092941	-0.029673	2.963215
150.489608	2905.166082	6.097946	-0.029714	2.967056
150.846351	2913.191581	6.102950	-0.029786	2.970894
151.019986	2921.267626	6.107955	-0.029823	2.974741
151.362533	2929.265759	6.112960	-0.029892	2.978555
151.843319	2937.296493	6.117965	-0.029986	2.982386
151.794812	2945.367097	6.122970	-0.029982	2.986205
152.338763	2953.352695	6.127974	-0.030089	2.990008
152.559784	2961.479584	6.132979	-0.030135	2.993857
152.798862	2969.462132	6.137984	-0.030185	2.997633
153.017112	2977.504830	6.142989	-0.030230	3.001432
153.208019	2985.504278	6.147994	-0.030271	3.005205
153.518985	2993.524518	6.152998	-0.030334	3.008989
153.758037	3001.593203	6.158003	-0.030384	3.012787
153.997280	3009.644851	6.163008	-0.030433	3.016572
154.600432	3017.639950	6.168013	-0.030551	3.020343
154.785818	3025.670971	6.173018	-0.030590	3.024107
155.070111	3033.707137	6.178022	-0.030648	3.027872
155.392137	3041.782362	6.183027	-0.030713	3.031653
155.768758	3049.805825	6.188032	-0.030789	3.035408
156.230845	3057.801011	6.193037	-0.030880	3.039149
156.770526	3065.816419	6.198042	-0.030985	3.042899
157.036287	3073.862894	6.203046	-0.031040	3.046645
157.368081	3081.916652	6.208051	-0.031107	3.050393
157.521202	3089.996857	6.213056	-0.031140	3.054140
157.969492	3098.022963	6.218061	-0.031229	3.057871
158.241683	3106.047393	6.223066	-0.031285	3.061589
158.331528	3114.065835	6.228070	-0.031306	3.065291
158.744733	3122.108473	6.233075	-0.031388	3.069014
158.724301	3130.215491	6.238080	-0.031390	3.072743
159.000369	3138.288586	6.243085	-0.031446	3.076465
159.107627	3146.279830	6.248090	-0.031471	3.080137
159.281821	3154.286156	6.253094	-0.031509	3.083815
159.526378	3162.305251	6.258099	-0.031559	3.087497
159.445493	3170.355981	6.263104	-0.031549	3.091174
159.876474	3178.376308	6.268109	-0.031635	3.094857
160.110371	3186.394735	6.273114	-0.031683	3.098526
160.339471	3194.428758	6.278118	-0.031731	3.102196
160.598524	3202.468045	6.283123	-0.031784	3.105867
160.619661	3210.509844	6.288128	-0.031793	3.109523
160.771907	3218.555610	6.293133	-0.031827	3.113182
160.950810	3226.604827	6.298138	-0.031865	3.116840
161.324886	3234.599365	6.303142	-0.031940	3.120478
161.523076	3242.625021	6.308147	-0.031982	3.124118
161.451999	3250.661919	6.313152	-0.031974	3.127746
161.847692	3258.715285	6.318157	-0.032053	3.131399
161.995365	3266.750059	6.323162	-0.032085	3.135027
162.214445	3274.780258	6.328166	-0.032131	3.138653
162.654894	3282.808530	6.333171	-0.032218	3.142283
162.743364	3290.811984	6.338176	-0.032240	3.145883
162.880596	3298.873488	6.343181	-0.032270	3.149506
163.210458	3306.940176	6.348186	-0.032337	3.153136
163.576170	3314.959111	6.353190	-0.032410	3.156742
163.927781	3322.946164	6.358195	-0.032481	3.160329
164.023355	3330.967327	6.363200	-0.032503	3.163916
164.440395	3338.977007	6.368205	-0.032586	3.167507
164.545721	3347.059775	6.373210	-0.032611	3.171114
164.613414	3355.082453	6.378214	-0.032629	3.174688
165.000703	3363.126996	6.383219	-0.032706	3.178281
165.441817	3371.118700	6.388224	-0.032793	3.181849
165.719934	3379.130303	6.393229	-0.032850	3.185415
165.782513	3387.206904	6.398234	-0.032867	3.188997
166.057159	3395.248372	6.403238	-0.032923	3.192568
166.442612	3403.304677	6.408243	-0.033000	3.196146
166.578393	3411.282907	6.413248	-0.033030	3.199675
166.700773	3419.332188	6.418253	-0.033058	3.203231
167.101523	3427.381833	6.423258	-0.033138	3.206795
167.312783	3435.381905	6.428262	-0.033182	3.210325
167.633428	3443.432438	6.433267	-0.033247	3.213878
167.858927	3451.477531	6.438272	-0.033294	3.217420
168.241795	3459.482646	6.443277	-0.033370	3.220948
168.568437	3467.481331	6.448282	-0.033436	3.224466
168.724276	3475.533445	6.453286	-0.033470	3.227997
169.057275	3483.613639	6.458291	-0.033537	3.231544
169.089161	3491.683017	6.463296	-0.033548	3.235069
169.434021	3499.679140	6.468301	-0.033618	3.238572
169.661873	3507.680616	6.473306	-0.033665	3.242068
170.248718	3515.649000	6.478310	-0.033779	3.245561
170.644150	3523.683452	6.483315	-0.033858	3.249071
170.893939	3531.723681	6.488320	-0.033910	3.252573
171.181596	3539.786499	6.493325	-0.033968	3.256083
171.254403	3547.792851	6.498330	-0.033987	3.259557
171.720332	3555.786922	6.503334	-0.034079	3.263036
172.404246	3563.825444	6.508339	-0.034211	3.266540
172.567033	3571.872033	6.513344	-0.034247	3.270023
172.793197	3579.940336	6.518349	-0.034294	3.273514
173.246091	3587.964897	6.523354	-0.034383	3.276991
173.509226	3595.971888	6.528358	-0.034437	3.280450
173.836628	3603.996898	6.533363	-0.034503	3.283915
174.000272	3612.053322	6.538368	-0.034539	3.287384
174.278348	3620.080388	6.543373	-0.034596	3.290840
174.216838	3628.149459	6.548378	-0.034590	3.294298
174.781131	3636.150465	6.553382	-0.034700	3.297747
175.112181	3644.203621	6.558387	-0.034766	3.301206
175.211410	3652.175746	6.563392	-0.034790	3.304618
175.383642	3660.241093	6.568397	-0.034827	3.308069
175.704877	3668.291460	6.573402	-0.034892	3.311515
175.837991	3676.335537	6.578406	-0.034922	3.314948
176.041404	3684.354655	6.583411	-0.034965	3.318369
176.374907	3692.335411	6.588416	-0.035032	3.321776
176.714907	3700.323953	6.593421	-0.035100	3.325182
176.788770	3708.376635	6.598426	-0.035119	3.328602
176.906153	3716.435298	6.603430	-0.035146	3.332023
177.263698	3724.478340	6.608435	-0.035218	3.335443
177.484600	3732.481941	6.613440	-0.035264	3.338837
177.643847	3740.507300	6.618445	-0.035299	3.342235
178.042281	3748.514938	6.623450	-0.035378	3.345630
178.420625	3756.547462	6.628454	-0.035454	3.349032
178.598450	3764.624226	6.633459	-0.035492	3.352441
178.931364	3772.646194	6.638464	-0.035559	3.355830
179.267854	3780.641957	6.643469	-0.035627	3.359204
179.449490	3788.670388	6.648474	-0.035665	3.362583
179.575822	3796.687167	6.653478	-0.035694	3.365952
179.885649	3804.744776	6.658483	-0.035757	3.369341
180.299057	3812.770484	6.663488	-0.035839	3.372717
180.595099	3820.829365	6.668493	-0.035899	3.376099
180.787589	3828.825305	6.673498	-0.035940	3.379447
180.963644	3836.838895	6.678502	-0.035978	3.382799
181.258851	3844.896876	6.683507	-0.036038	3.386171
181.385773	3852.921014	6.688512	-0.036067	3.389519
181.602663	3861.011609	6.693517	-0.036112	3.392894
181.781679	3869.073744	6.698522	-0.036151	3.396253
182.027646	3877.012032	6.703526	-0.036201	3.399560
182.230517	3885.009937	6.708531	-0.036244	3.402886
182.497098	3893.027783	6.713536	-0.036299	3.406220
182.832730	3901.044099	6.718541	-0.036366	3.409552
183.126187	3909.085510	6.723546	-0.036426	3.412890
183.213198	3917.142971	6.728550	-0.036448	3.416224
183.314682	3925.155727	6.733555	-0.036471	3.419537
183.582852	3933.164837	6.738560	-0.036526	3.422850
183.768263	3941.203802	6.743565	-0.036566	3.426170
183.937726	3949.240589	6.748570	-0.036603	3.429486
184.369248	3957.241012	6.753574	-0.036688	3.432791
184.613636	3965.326956	6.758579	-0.036739	3.436123
184.845090	3973.291078	6.763584	-0.036787	3.439401
184.949025	3981.341043	6.768589	-0.036811	3.442706
185.267151	3989.344090	6.773594	-0.036876	3.445997
185.379522	3997.393705	6.778598	-0.036902	3.449296
185.651059	4005.436718	6.783603	-0.036957	3.452595
185.858829	4013.468228	6.788608	-0.037001	3.455883
186.343565	4021.482195	6.793613	-0.037096	3.459171
186.466821	4029.520717	6.798618	-0.037124	3.462453
186.518777	4037.529699	6.803622	-0.037139	3.465718
187.030821	4045.570978	6.808627	-0.037240	3.469008
186.957167	4053.629071	6.813632	-0.037231	3.472283
187.072853	4061.671269	6.818637	-0.037258	3.475554
187.369906	4069.658277	6.823642	-0.037318	3.478806
187.590543	4077.658932	6.828646	-0.037364	3.482057
187.772227	4085.677180	6.833651	-0.037403	3.485312
187.934570	4093.697586	6.838656	-0.037438	3.488563
188.276746	4101.741592	6.843661	-0.037507	3.491827
188.513868	4109.770574	6.848666	-0.037556	3.495078
188.647303	4117.782731	6.853670	-0.037586	3.498316
188.967555	4125.803343	6.858675	-0.037651	3.501561
189.277030	4133.755632	6.863680	-0.037714	3.504774
189.631321	4141.822869	6.868685	-0.037785	3.508032
189.981157	4149.867828	6.873690	-0.037855	3.511278
190.304997	4157.885083	6.878694	-0.037920	3.514509
190.390989	4165.945253	6.883699	-0.037941	3.517747
190.581675	4173.944124	6.888704	-0.037982	3.520961
190.895989	4181.928479	6.893709	-0.038046	3.524169
191.371868	4189.987544	6.898714	-0.038139	3.527409
191.622997	4198.004156	6.903718	-0.038191	3.530623
191.899218	4206.074761	6.908723	-0.038248	3.533856
192.307348	4214.107705	6.913728	-0.038329	3.537075
192.425922	4222.129271	6.918733	-0.038356	3.540277
192.739126	4230.138817	6.923738	-0.038419	3.543478
192.964154	4238.168647	6.928742	-0.038466	3.546681
193.271537	4246.205967	6.933747	-0.038529	3.549887
193.443146	4254.318215	6.938752	-0.038566	3.553115
193.786236	4262.355927	6.943757	-0.038635	3.556316
194.301337	4270.279599	6.948762	-0.038736	3.559474
194.346780	4278.300498	6.953766	-0.038749	3.562654
194.650472	4286.303207	6.958771	-0.038811	3.565831
194.728192	4294.335371	6.963776	-0.038830	3.569010
194.964111	4302.386036	6.968781	-0.038879	3.572199
195.053708	4310.434162	6.973786	-0.038901	3.575379
195.240505	4318.395309	6.978790	-0.038941	3.578525
195.487160	4326.481225	6.983795	-0.038992	3.581719
195.611667	4334.431865	6.988800	-0.039020	3.584854
195.880760	4342.465574	6.993805	-0.039075	3.588022
196.132503	4350.501412	6.998810	-0.039127	3.591188
196.235701	4358.529724	7.003814	-0.039152	3.594345
196.234853	4366.614016	7.008819	-0.039157	3.597517
196.459390	4374.559433	7.013824	-0.039203	3.600638
196.801632	4382.551274	7.018829	-0.039272	3.603778
196.953847	4390.635626	7.023834	-0.039306	3.606946
197.170279	4398.613963	7.028838	-0.039351	3.610072
197.595066	4406.682073	7.033843	-0.039435	3.613236
197.628085	4414.727554	7.038848	-0.039446	3.616377
197.715543	4422.701732	7.043853	-0.039468	3.619490
198.136606	4430.729888	7.048858	-0.039551	3.622630
198.242603	4438.740777	7.053862	-0.039576	3.625751
198.553120	4446.795706	7.058867	-0.039639	3.628893
198.612095	4454.861648	7.063872	-0.039655	3.632029
198.746333	4462.910055	7.068877	-0.039685	3.635158
198.848386	4470.913758	7.073882	-0.039709	3.638266
199.142624	4478.900588	7.078886	-0.039769	3.641370
199.523046	4486.893264	7.083891	-0.039845	3.644476
199.569983	4494.955424	7.088896	-0.039859	3.647597
199.920249	4502.948779	7.093901	-0.039929	3.650697
200.285506	4511.026492	7.098906	-0.040002	3.653827
200.338212	4519.041988	7.103910	-0.040017	3.656922
200.452329	4527.060938	7.108915	-0.040043	3.660017
200.700475	4535.068730	7.113920	-0.040095	3.663109
201.038671	4543.093541	7.118925	-0.040163	3.666208
201.206964	4551.120515	7.123930	-0.040199	3.669300
201.254333	4559.152719	7.128934	-0.040213	3.672388
201.536018	4567.189018	7.133939	-0.040271	3.675481
201.620060	4575.185192	7.138944	-0.040291	3.678551
201.977785	4583.191849	7.143949	-0.040363	3.681630
202.205687	4591.209107	7.148954	-0.040410	3.684707
202.329497	4599.209059	7.153958	-0.040439	3.687772
202.614499	4607.259804	7.158963	-0.040497	3.690857
202.729321	4615.309009	7.163968	-0.040523	3.693936
203.061385	4623.345812	7.168973	-0.040590	3.697012
203.294138	4631.335373	7.173978	-0.040638	3.700066
203.467900	4639.345328	7.178982	-0.040676	3.703123
203.567352	4647.377485	7.183987	-0.040700	3.706184
203.641392	4655.420444	7.188992	-0.040718	3.709246
203.866581	4663.479206	7.193997	-0.040765	3.712315
204.326163	4671.557583	7.199002	-0.040856	3.715395
204.536561	4679.459751	7.204006	-0.040900	3.718399
204.784434	4687.564492	7.209011	-0.040952	3.721479
205.038513	4695.467948	7.214016	-0.041004	3.724480
205.354525	4703.505940	7.219021	-0.041068	3.727530
205.780520	4711.524689	7.224026	-0.041152	3.730574
205.867643	4719.587341	7.229030	-0.041174	3.733624
206.249299	4727.605783	7.234035	-0.041250	3.736661
206.381395	4735.581246	7.239040	-0.041279	3.739674
206.419944	4743.644453	7.244045	-0.041292	3.742715
206.940719	4751.657551	7.249050	-0.041394	3.745746
207.319597	4759.642250	7.254054	-0.041469	3.748761
207.316049	4767.742018	7.259059	-0.041474	3.751807
207.402183	4775.758051	7.264064	-0.041495	3.754822
207.771824	4783.769713	7.269069	-0.041569	3.757839
207.842827	4791.804706	7.274074	-0.041587	3.760855
207.909130	4799.786496	7.279078	-0.041604	3.763849
208.190463	4807.837389	7.284083	-0.041662	3.766872
208.336622	4815.829696	7.289088	-0.041694	3.769867
208.536747	4823.908655	7.294093	-0.041737	3.772893
208.850372	4831.943859	7.299098	-0.041800	3.775903
209.331847	4839.916095	7.304102	-0.041895	3.778890
209.655423	4847.978865	7.309107	-0.041960	3.781906
209.617505	4855.969381	7.314112	-0.041958	3.784884
209.957189	4864.033305	7.319117	-0.042026	3.787896
210.213209	4872.040824	7.324122	-0.042079	3.790882
210.296797	4880.069221	7.329126	-0.042100	3.793870
210.480735	4888.135865	7.334131	-0.042139	3.796871
210.705572	4896.066944	7.339136	-0.042186	3.799821
210.793380	4904.087269	7.344141	-0.042207	3.802799
211.102602	4912.104310	7.349146	-0.042270	3.805778
211.214505	4920.115701	7.354150	-0.042296	3.808748
211.393282	4928.201224	7.359155	-0.042334	3.811745
211.429691	4936.172267	7.364160	-0.042346	3.814694
211.673747	4944.211005	7.369165	-0.042397	3.817670
211.811403	4952.214904	7.374170	-0.042427	3.820629
212.019745	4960.206623	7.379174	-0.042471	3.823583
212.485534	4968.259327	7.384179	-0.042563	3.826562
212.622596	4976.279638	7.389184	-0.042594	3.829519
212.773950	4984.355458	7.394189	-0.042627	3.832496
213.017278	4992.344114	7.399194	-0.042677	3.835439
213.163108	5000.321586	7.404198	-0.042710	3.838375
213.411023	5008.365813	7.409203	-0.042761	3.841334
213.680549	5016.358127	7.414208	-0.042816	3.844273
214.066939	5024.374844	7.419213	-0.042893	3.847221
214.181073	5032.441182	7.424218	-0.042919	3.850179
214.356583	5040.464310	7.429222	-0.042957	3.853120
214.455513	5048.518377	7.434227	-0.042981	3.856069
214.821214	5056.517816	7.439232	-0.043054	3.859001
214.939849	5064.518269	7.444237	-0.043081	3.861926
215.070420	5072.562695	7.449242	-0.043110	3.864865
215.223590	5080.572686	7.454246	-0.043144	3.867790
215.691770	5088.597396	7.459251	-0.043236	3.870724
215.665290	5096.826711	7.464256	-0.043237	3.873720
215.969045	5104.837738	7.469261	-0.043298	3.876641
216.501809	5112.755883	7.474266	-0.043402	3.879531
216.359120	5120.721514	7.479270	-0.043381	3.882423
216.705077	5128.710810	7.484275	-0.043450	3.885330
216.705099	5136.729812	7.489280	-0.043455	3.888240
216.928685	5144.760208	7.494285	-0.043502	3.891155
217.138228	5152.801782	7.499290	-0.043546	3.894072
217.534105	5160.802582	7.504294	-0.043625	3.896976
217.674974	5168.775403	7.509299	-0.043656	3.899863
217.958361	5176.827114	7.514304	-0.043714	3.902778
218.180754	5184.816376	7.519309	-0.043761	3.905668
218.660826	5192.864070	7.524314	-0.043855	3.908582
218.668669	5200.879144	7.529318	-0.043862	3.911472
218.892665	5208.953172	7.534323	-0.043908	3.914386
219.064288	5216.971822	7.539328	-0.043945	3.917277
219.207056	5224.914625	7.544333	-0.043977	3.920137
219.555504	5232.948382	7.549338	-0.044047	3.923032
219.647012	5240.944746	7.554342	-0.044069	3.925907
219.974571	5248.984686	7.559347	-0.044135	3.928800
219.956137	5257.007177	7.564352	-0.044137	3.931678
220.288637	5265.035396	7.569357	-0.044204	3.934562
220.660649	5273.110402	7.574362	-0.044278	3.937461
220.679330	5281.075595	7.579366	-0.044287	3.940313
220.882177	5289.102939	7.584371	-0.044330	3.943188
221.100529	5297.101396	7.589376	-0.044375	3.946051
221.269918	5305.137020	7.594381	-0.044412	3.948924
221.371110	5313.195909	7.599386	-0.044436	3.951802
221.731554	5321.219200	7.604390	-0.044508	3.954670
222.146424	5329.238825	7.609395	-0.044590	3.957535
222.147861	5337.205497	7.614400	-0.044596	3.960373
222.393752	5345.217902	7.619405	-0.044647	3.963228
222.616002	5353.247868	7.624410	-0.044693	3.966088
222.923308	5361.273518	7.629414	-0.044755	3.968945
222.847810	5369.319769	7.634419	-0.044746	3.971801
222.985097	5377.350271	7.639424	-0.044777	3.974653
223.290820	5385.371619	7.644429	-0.044839	3.977502
223.507884	5393.386271	7.649434	-0.044884	3.980346
223.571936	5401.390093	7.654438	-0.044901	3.983181
223.974566	5409.389182	7.659443	-0.044982	3.986018
224.086836	5417.449125	7.664448	-0.045008	3.988870
224.370760	5425.455696	7.669453	-0.045065	3.991703
224.571924	5433.522309	7.674458	-0.045108	3.994554
224.647685	5441.504033	7.679462	-0.045127	3.997372
224.708771	5449.516898	7.684467	-0.045144	4.000198
225.001749	5457.541777	7.689472	-0.045203	4.003030
225.099260	5465.536952	7.694477	-0.045226	4.005846
225.241912	5473.591694	7.699482	-0.045258	4.008682
225.530573	5481.592365	7.704486	-0.045317	4.011499
226.005884	5489.649134	7.709491	-0.045411	4.014337
226.176044	5497.666652	7.714496	-0.045447	4.017155
226.247341	5505.621249	7.719501	-0.045466	4.019946
226.309290	5513.686946	7.724506	-0.045482	4.022775
226.444783	5521.683809	7.729510	-0.045513	4.025578
226.502048	5529.725409	7.734515	-0.045528	4.028394
226.970587	5537.748550	7.739520	-0.045621	4.031208
227.167038	5545.851805	7.744525	-0.045662	4.034044
227.197842	5553.916132	7.749530	-0.045673	4.036862
227.461201	5561.795430	7.754534	-0.045727	4.039616
227.891283	5569.802918	7.759539	-0.045812	4.042416
228.065092	5577.795674	7.764544	-0.045850	4.045205
227.959217	5585.838124	7.769549	-0.045835	4.048005
228.503608	5593.851562	7.774554	-0.045942	4.050803
228.482222	5601.879213	7.779558	-0.045943	4.053595
228.672686	5609.934110	7.784563	-0.045983	4.056398
228.810462	5617.899759	7.789568	-0.046014	4.059167
229.132152	5625.910096	7.794573	-0.046079	4.061952
229.127743	5633.915171	7.799578	-0.046083	4.064730
229.134598	5641.950490	7.804582	-0.046089	4.067515
229.647924	5649.977013	7.809587	-0.046190	4.070303
229.763429	5658.033501	7.814592	-0.046217	4.073094
229.899952	5666.050490	7.819597	-0.046247	4.075869
230.267019	5674.037557	7.824602	-0.046321	4.078636
230.364883	5682.074405	7.829606	-0.046344	4.081414
230.642974	5690.040864	7.834611	-0.046401	4.084168
230.889229	5698.076542	7.839616	-0.046452	4.086944
230.926380	5706.049027	7.844621	-0.046464	4.089693
231.320883	5714.154309	7.849626	-0.046542	4.092491
231.417773	5722.169872	7.854630	-0.046565	4.095252
231.562464	5730.210824	7.859635	-0.046597	4.098021
231.662275	5738.169999	7.864640	-0.046621	4.100759
231.781009	5746.164718	7.869645	-0.046648	4.103507
231.992807	5754.239518	7.874650	-0.046693	4.106283
232.358770	5762.220275	7.879654	-0.046766	4.109026
232.510390	5770.354882	7.884659	-0.046799	4.111817
232.677599	5778.362352	7.889664	-0.046835	4.114564
232.945219	5786.371491	7.894669	-0.046890	4.117310
233.056301	5794.314350	7.899674	-0.046916	4.120029
233.041972	5802.376736	7.904678	-0.046919	4.122786
233.290779	5810.379088	7.909683	-0.046970	4.125524
233.694901	5818.378434	7.914688	-0.047050	4.128261
234.025191	5826.394188	7.919693	-0.047117	4.131001
234.272321	5834.471529	7.924698	-0.047168	4.133759
234.653734	5842.484480	7.929702	-0.047244	4.136495
234.801178	5850.487447	7.934707	-0.047277	4.139223
234.907997	5858.488035	7.939712	-0.047301	4.141947
235.128132	5866.486251	7.944717	-0.047348	4.144671
235.517782	5874.585827	7.949722	-0.047425	4.147429
235.553459	5882.552603	7.954726	-0.047437	4.150135
235.774388	5890.600937	7.959731	-0.047483	4.152870
235.936416	5898.643829	7.964736	-0.047518	4.155601
235.996481	5906.619145	7.969741	-0.047535	4.158305
236.284709	5914.653619	7.974746	-0.047593	4.161031
236.420428	5922.615673	7.979750	-0.047624	4.163728
236.544608	5930.663643	7.984755	-0.047652	4.166453
236.923851	5938.667705	7.989760	-0.047728	4.169164
237.043714	5946.691376	7.994765	-0.047755	4.171876
237.199677	5954.768137	7.999770	-0.047789	4.174606
237.236059	5962.743167	8.004774	-0.047801	4.177297
237.374839	5970.744068	8.009779	-0.047832	4.179997
237.535695	5978.784694	8.014784	-0.047867	4.182709
237.704107	5986.747844	8.019789	-0.047903	4.185393
238.076266	5994.792167	8.024794	-0.047978	4.188105
238.395463	6002.818499	8.029798	-0.048042	4.190808
238.819459	6010.925772	8.034803	-0.048126	4.193538
238.925455	6018.959362	8.039808	-0.048151	4.196238
238.969234	6026.864324	8.044813	-0.048164	4.198892
239.150641	6034.931961	8.049818	-0.048203	4.201601
239.219912	6042.881706	8.054822	-0.048221	4.204267
240.053062	6050.894891	8.059827	-0.048381	4.206961
241.499152	6058.884442	8.064832	-0.048656	4.209651
241.625742	6066.894853	8.069837	-0.048684	4.212333
242.196270	6075.000603	8.074842	-0.048796	4.215049
242.375658	6082.978783	8.079846	-0.048834	4.217717
242.696884	6090.971868	8.084851	-0.048899	4.220390
242.953545	6099.020737	8.089856	-0.048952	4.223079
243.139115	6106.969279	8.094861	-0.048991	4.225732
243.425606	6115.043600	8.099866	-0.049050	4.228426
243.457955	6123.070619	8.104870	-0.049061	4.231101
243.567782	6131.117375	8.109875	-0.049086	4.233781
243.637694	6139.176063	8.114880	-0.049105	4.236462
243.795418	6147.138756	8.119885	-0.049139	4.239111
243.958684	6155.172134	8.124890	-0.049174	4.241782
244.194993	6163.077863	8.129894	-0.049223	4.244410
244.226987	6171.221115	8.134899	-0.049235	4.247113
244.466240	6179.199015	8.139904	-0.049284	4.249761
244.577301	6187.244900	8.144909	-0.049310	4.252428
244.761161	6195.247692	8.149914	-0.049349	4.255081
244.839924	6203.315031	8.154918	-0.049369	4.257752
245.103670	6211.248417	8.159923	-0.049423	4.260379
245.324121	6219.313610	8.164928	-0.049469	4.263047
245.470218	6227.297087	8.169933	-0.049502	4.265686
245.750508	6235.376600	8.174938	-0.049559	4.268357
245.943696	6243.371784	8.179942	-0.049600	4.270997
246.272487	6251.441380	8.184947	-0.049666	4.273661
246.150139	6259.482349	8.189952	-0.049648	4.276310
246.282540	6267.419313	8.194957	-0.049678	4.278925
246.481190	6275.478098	8.199962	-0.049720	4.281579
246.628878	6283.411302	8.204966	-0.049753	4.284190
246.735561	6291.488182	8.209971	-0.049778	4.286846
246.992560	6299.477977	8.214976	-0.049831	4.289473
247.191860	6307.560759	8.219981	-0.049873	4.292129
247.463857	6315.546923	8.224986	-0.049929	4.294752
247.566933	6323.621237	8.229990	-0.049953	4.297401
247.537894	6331.567509	8.234995	-0.049952	4.300005
247.457877	6339.595137	8.240000	-0.049943	4.302633
247.645284	6347.572641	8.245005	-0.049983	4.305246
247.990757	6355.606718	8.250010	-0.050052	4.307877
247.861303	6363.612054	8.255014	-0.050033	4.310493
248.336004	6371.693278	8.260019	-0.050126	4.313137
248.442229	6379.691529	8.265024	-0.050151	4.315750
248.603946	6387.680971	8.270029	-0.050186	4.318358
248.514306	6395.710678	8.275034	-0.050175	4.320976
248.830468	6403.653739	8.280038	-0.050239	4.323568
249.065098	6411.731978	8.285043	-0.050288	4.326201
249.219567	6419.756568	8.290048	-0.050321	4.328814
249.422876	6427.763894	8.295053	-0.050364	4.331421
249.720250	6435.820203	8.300058	-0.050425	4.334042
249.632712	6443.840745	8.305062	-0.050414	4.336648
249.816404	6451.779549	8.310067	-0.050453	4.339227
250.248841	6459.840129	8.315072	-0.050538	4.341846
250.350375	6467.778821	8.320077	-0.050562	4.344422
250.527446	6475.857513	8.325082	-0.050600	4.347042
250.585834	6483.870322	8.330086	-0.050616	4.349638
250.978355	6491.942915	8.335091	-0.050695	4.352254
251.147654	6500.019216	8.340096	-0.050731	4.354869
251.122967	6507.979720	8.345101	-0.050732	4.357443
251.580398	6515.965403	8.350106	-0.050822	4.360027
251.804591	6523.956687	8.355110	-0.050869	4.362609
251.809745	6531.931870	8.360115	-0.050875	4.365184
252.046006	6539.955763	8.365120	-0.050924	4.367774
252.038577	6547.962970	8.370125	-0.050927	4.370355
252.415216	6556.037519	8.375130	-0.051003	4.372959
252.473594	6564.075407	8.380134	-0.051019	4.375548
252.666417	6572.070020	8.385139	-0.051060	4.378122
252.654165	6580.077989	8.390144	-0.051062	4.380698
252.797018	6588.045149	8.395149	-0.051094	4.383260
253.087066	6596.121355	8.400154	-0.051153	4.385856
253.291792	6604.128098	8.405158	-0.051196	4.388428
253.451115	6612.157931	8.410163	-0.051231	4.391005
253.565510	6620.224485	8.415168	-0.051257	4.393593
253.605084	6628.200652	8.420173	-0.051270	4.396149
253.850229	6636.186817	8.425178	-0.051321	4.398709
253.883117	6644.209541	8.430182	-0.051332	4.401277
254.357177	6652.189737	8.435187	-0.051425	4.403833
254.503609	6660.234753	8.440192	-0.051457	4.406406
254.612640	6668.269497	8.445197	-0.051483	4.408974
254.929763	6676.341877	8.450202	-0.051547	4.411554
254.999025	6684.346659	8.455206	-0.051565	4.414109
255.172430	6692.379967	8.460211	-0.051602	4.416673
255.255781	6700.334166	8.465216	-0.051623	4.419209
255.682750	6708.332909	8.470221	-0.051707	4.421760
255.954454	6716.365223	8.475226	-0.051763	4.424319
256.041342	6724.394207	8.480230	-0.051784	4.426875
256.144015	6732.404082	8.485235	-0.051809	4.429423
256.398156	6740.469515	8.490240	-0.051861	4.431988
256.498740	6748.462259	8.495245	-0.051885	4.434528
256.938103	6756.550357	8.500250	-0.051972	4.437098
256.995681	6764.495004	8.505254	-0.051987	4.439619
257.251143	6772.564625	8.510259	-0.052040	4.442179
257.433055	6780.517813	8.515264	-0.052079	4.444701
257.580272	6788.533226	8.520269	-0.052112	4.447241
257.909636	6796.529247	8.525274	-0.052178	4.449774
257.789288	6804.589931	8.530278	-0.052161	4.452324
258.093577	6812.586708	8.535283	-0.052222	4.454854
258.090740	6820.659113	8.540288	-0.052227	4.457405
258.300911	6828.577373	8.545293	-0.052271	4.459907
258.450253	6836.696755	8.550298	-0.052304	4.462471
258.505830	6844.622031	8.555302	-0.052319	4.464972
258.784611	6852.675981	8.560307	-0.052376	4.467512
259.024335	6860.706339	8.565312	-0.052426	4.470044
258.977669	6868.733620	8.570317	-0.052422	4.472572
259.124890	6876.770264	8.575322	-0.052455	4.475102
259.389484	6884.783466	8.580327	-0.052509	4.477624
259.575573	6892.725648	8.585331	-0.052549	4.480122
259.791825	6900.725694	8.590336	-0.052594	4.482637
259.790714	6908.731529	8.595341	-0.052599	4.485152
259.913511	6916.815249	8.600346	-0.052627	4.487689
260.460561	6924.824818	8.605351	-0.052734	4.490204
260.722509	6932.807953	8.610355	-0.052788	4.492708
260.592381	6940.871064	8.615360	-0.052769	4.495234
260.715289	6948.855588	8.620365	-0.052797	4.497735
261.093683	6956.870262	8.625370	-0.052872	4.500245
261.115167	6964.887698	8.630375	-0.052881	4.502753
261.516162	6972.882402	8.635379	-0.052961	4.505254
261.654864	6980.927878	8.640384	-0.052992	4.507768
261.685907	6988.908793	8.645389	-0.053003	4.510261
261.952616	6997.021326	8.650394	-0.053058	4.512794
261.915725	7005.017762	8.655399	-0.053056	4.515288
262.179196	7012.992297	8.660403	-0.053110	4.517775
262.363223	7020.999983	8.665408	-0.053149	4.520271
262.681331	7028.963081	8.670413	-0.053213	4.522752
262.920304	7036.968357	8.675418	-0.053263	4.525244
262.845301	7045.030475	8.680423	-0.053254	4.527752
263.138796	7053.012246	8.685427	-0.053314	4.530234
263.383680	7061.080231	8.690432	-0.053365	4.532742
263.572221	7069.070685	8.695437	-0.053405	4.535224
263.756033	7077.132027	8.700442	-0.053444	4.537726
263.880922	7085.104625	8.705447	-0.053472	4.540200
263.858289	7093.136847	8.710451	-0.053473	4.542690
264.166016	7101.176717	8.715456	-0.053536	4.545182
264.440653	7109.164836	8.720461	-0.053592	4.547657
264.628797	7117.163911	8.725466	-0.053632	4.550133
264.743667	7125.229354	8.730471	-0.053658	4.552629
264.983416	7133.230016	8.735475	-0.053708	4.555103
265.372288	7141.274885	8.740480	-0.053786	4.557589
265.119430	7149.200661	8.745485	-0.053744	4.560037
265.422790	7157.320546	8.750490	-0.053805	4.562544
265.624954	7165.266261	8.755495	-0.053848	4.564996
265.705160	7173.340335	8.760499	-0.053868	4.567486
266.014487	7181.282274	8.765504	-0.053930	4.569934
266.143337	7189.350854	8.770509	-0.053960	4.572419
266.431008	7197.379772	8.775514	-0.054018	4.574891
266.321256	7205.407201	8.780519	-0.054003	4.577361
266.521099	7213.349743	8.785523	-0.054045	4.579803
267.009805	7221.411714	8.790528	-0.054141	4.582282
267.160162	7229.405837	8.795533	-0.054174	4.584737
267.106530	7237.447466	8.800538	-0.054169	4.587206
267.252350	7245.427896	8.805543	-0.054202	4.589655
267.461936	7253.490948	8.810547	-0.054246	4.592128
267.389744	7261.550718	8.815552	-0.054237	4.594599
267.691239	7269.574549	8.820557	-0.054299	4.597057
268.099023	7277.545563	8.825562	-0.054380	4.599498
268.299366	7285.554850	8.830567	-0.054422	4.601949
268.221819	7293.505401	8.835571	-0.054412	4.604381
268.526055	7301.584545	8.840576	-0.054474	4.606850
268.678304	7309.532268	8.845581	-0.054508	4.609279
268.654633	7317.643812	8.850586	-0.054508	4.611756
268.787967	7325.651260	8.855591	-0.054538	4.614200
269.111291	7333.666124	8.860595	-0.054604	4.616644
269.290937	7341.645364	8.865600	-0.054642	4.619077
269.347758	7349.649310	8.870605	-0.054658	4.621516
269.641940	7357.666932	8.875610	-0.054718	4.623958
269.671608	7365.681468	8.880615	-0.054728	4.626397
269.751823	7373.693129	8.885619	-0.054748	4.628835
270.004278	7381.768857	8.890624	-0.054800	4.631290
270.005666	7389.741713	8.895629	-0.054806	4.633713
270.304786	7397.823117	8.900634	-0.054866	4.636167
270.375802	7405.768582	8.905639	-0.054885	4.638580
270.770809	7413.797136	8.910643	-0.054963	4.641015
270.862813	7421.808759	8.915648	-0.054985	4.643445
270.924175	7429.810120	8.920653	-0.055002	4.645870
271.212821	7437.845180	8.925658	-0.055061	4.648304
271.268687	7445.867384	8.930663	-0.055076	4.650733
271.530674	7453.884139	8.935667	-0.055130	4.653159
271.862042	7461.883736	8.940672	-0.055197	4.655578
271.974036	7469.887888	8.945677	-0.055223	4.657997
272.118433	7477.900508	8.950682	-0.055255	4.660418
272.099926	7485.899140	8.955687	-0.055256	4.662834
272.530053	7493.848928	8.960691	-0.055341	4.665233
272.668520	7501.976671	8.965696	-0.055372	4.667684
272.940161	7509.937418	8.970701	-0.055428	4.670084
273.040245	7518.058042	8.975706	-0.055452	4.672531
273.225508	7526.124289	8.980711	-0.055491	4.674961
273.178159	7534.114787	8.985715	-0.055488	4.677366
273.335831	7542.009797	8.990720	-0.055522	4.679741
273.588990	7549.996635	8.995725	-0.055574	4.682143
273.720249	7558.012961	9.000730	-0.055604	4.684552
273.971149	7566.068478	9.005735	-0.055655	4.686972
274.130002	7574.008099	9.010739	-0.055690	4.689355
274.445323	7582.108894	9.015744	-0.055754	4.691786
274.482439	7590.091454	9.020749	-0.055766	4.694180
274.797511	7598.143500	9.025754	-0.055830	4.696593
274.849499	7606.113599	9.030759	-0.055844	4.698981
274.938503	7614.158945	9.035763	-0.055866	4.701391
275.109134	7622.176710	9.040768	-0.055903	4.703790
275.408017	7630.153666	9.045773	-0.055964	4.706176
275.642732	7638.237695	9.050778	-0.056012	4.708593
275.701996	7646.216980	9.055783	-0.056028	4.710977
276.120155	7654.262803	9.060787	-0.056111	4.713380
276.199262	7662.328945	9.065792	-0.056131	4.715788
276.196913	7670.284494	9.070797	-0.056136	4.718162
276.374746	7678.272829	9.075802	-0.056174	4.720544
276.549468	7686.296673	9.080807	-0.056212	4.722935
276.582041	7694.289843	9.085811	-0.056223	4.725317
276.786803	7702.398753	9.090816	-0.056266	4.727731
277.197870	7710.352256	9.095821	-0.056348	4.730097
277.245643	7718.411400	9.100826	-0.056362	4.732494
277.397319	7726.417908	9.105831	-0.056395	4.734875
277.464198	7734.429768	9.110835	-0.056412	4.737255
278.085146	7742.396650	9.115840	-0.056533	4.739620
277.957074	7750.433633	9.120845	-0.056514	4.742007
278.242108	7758.392684	9.125850	-0.056572	4.744367
278.281264	7766.458466	9.130855	-0.056585	4.746759
278.483987	7774.476403	9.135859	-0.056628	4.749136
278.842110	7782.533898	9.140864	-0.056699	4.751522
278.959607	7790.567555	9.145869	-0.056726	4.753900
279.365047	7798.542138	9.150874	-0.056807	4.756259
279.299331	7806.548045	9.155879	-0.056800	4.758628
279.636235	7814.568000	9.160883	-0.056868	4.760998
279.864143	7822.583373	9.165888	-0.056915	4.763366
279.949942	7830.586280	9.170893	-0.056936	4.765730
280.161041	7838.606401	9.175898	-0.056980	4.768097
280.292978	7846.601019	9.180903	-0.057010	4.770456
280.441425	7854.601982	9.185907	-0.057043	4.772815
280.555702	7862.672198	9.190912	-0.057069	4.775194
280.787614	7870.673863	9.195917	-0.057117	4.777551
281.080240	7878.657066	9.200922	-0.057177	4.779900
280.988049	7886.712258	9.205927	-0.057165	4.782272
281.065585	7894.628361	9.210931	-0.057184	4.784601
281.304947	7902.739655	9.215936	-0.057234	4.786985
281.544133	7910.691471	9.220941	-0.057284	4.789321
281.775131	7918.774708	9.225946	-0.057332	4.791695
281.987625	7926.785206	9.230951	-0.057376	4.794046
282.031892	7934.857880	9.235955	-0.057390	4.796415
282.213063	7942.790780	9.240960	-0.057428	4.798741
282.326334	7950.826691	9.245965	-0.057455	4.801097
282.714149	7958.806896	9.250970	-0.057532	4.803433
282.650806	7966.823545	9.255975	-0.057525	4.805782
282.773207	7974.833168	9.260979	-0.057553	4.808126
283.166478	7982.901249	9.265984	-0.057631	4.810485
283.074607	7990.393292	9.270989	-0.057619	4.812677
283.276854	7995.013950	9.275994	-0.057660	4.814027
283.553343	7997.495347	9.280999	-0.057712	4.814751
283.799261	7998.822884	9.286003	-0.057759	4.815138
283.935761	7999.712863	9.291008	-0.057785	4.815397
283.817734	7999.677794	9.296013	-0.057763	4.815387
283.840384	7999.787121	9.301018	-0.057767	4.815419
283.932066	7999.739470	9.306023	-0.057784	4.815405
284.016521	7999.750459	9.311027	-0.057799	4.815408
284.132825	7999.921153	9.316032	-0.057821	4.815457
284.379128	8000.098259	9.321037	-0.057867	4.815508
284.409154	8000.083782	9.326042	-0.057872	4.815503
284.550625	8000.099982	9.331047	-0.057898	4.815507
284.609448	8000.001577	9.336051	-0.057909	4.815478
284.601151	7999.776005	9.341056	-0.057907	4.815412
284.703234	8000.057578	9.346061	-0.057926	4.815494
284.738353	7999.987630	9.351066	-0.057933	4.815473
284.804231	8000.021818	9.356071	-0.057945	4.815483
284.569651	8000.008335	9.361075	-0.057901	4.815480
284.833558	7999.961376	9.366080	-0.057950	4.815465
284.732649	8000.125301	9.371085	-0.057931	4.815514
284.894482	8000.042478	9.376090	-0.057961	4.815489
285.027491	8000.036104	9.381095	-0.057986	4.815486
284.950764	7999.930129	9.386099	-0.057971	4.815456
285.104656	7999.908072	9.391104	-0.058000	4.815449
285.031452	8000.038265	9.396109	-0.057986	4.815487
285.150434	7999.937644	9.401114	-0.058008	4.815457
285.162849	8000.029714	9.406119	-0.058010	4.815484
285.198929	7999.909568	9.411123	-0.058017	4.815449
285.228140	7999.926060	9.416128	-0.058022	4.815453
285.286260	8000.118241	9.421133	-0.058033	4.815509
285.274352	7999.966322	9.426138	-0.058030	4.815465
285.240648	7999.971097	9.431143	-0.058024	4.815466
285.598191	7999.931020	9.436147	-0.058090	4.815453
285.497281	8000.057553	9.441152	-0.058071	4.815490
285.519366	8000.096365	9.446157	-0.058075	4.815502
285.315648	8000.000054	9.451162	-0.058037	4.815474
285.434814	7999.996657	9.456167	-0.058059	4.815473
285.280699	7999.935350	9.461171	-0.058030	4.815456
285.430886	8000.021138	9.466176	-0.058058	4.815480
285.277995	8000.096604	9.471181	-0.058030	4.815503
285.290932	7999.994238	9.476186	-0.058032	4.815473
285.569783	8000.034065	9.481191	-0.058084	4.815483
285.498506	7999.980529	9.486195	-0.058070	4.815468
285.654957	7999.870907	9.491200	-0.058099	4.815435
285.404300	8000.056946	9.496205	-0.058052	4.815491
285.674696	8000.072061	9.501210	-0.058102	4.815494
285.671728	7999.880758	9.506215	-0.058102	4.815438
285.479261	7999.901086	9.511219	-0.058066	4.815445
285.741058	7999.970547	9.516224	-0.058114	4.815464
285.847346	7999.933818	9.521229	-0.058134	4.815453
285.609143	7999.937368	9.526234	-0.058089	4.815455
285.660052	8000.019389	9.531239	-0.058099	4.815478
285.719702	7999.931680	9.536243	-0.058110	4.815453
285.677593	7999.830547	9.541248	-0.058102	4.815423
285.525427	7999.930597	9.546253	-0.058073	4.815453
285.894871	7999.978323	9.551258	-0.058142	4.815465
285.676820	7999.845451	9.556263	-0.058101	4.815428
285.643651	7999.914337	9.561267	-0.058095	4.815448
285.863847	7999.855977	9.566272	-0.058136	4.815430
285.640730	7999.935630	9.571277	-0.058094	4.815454
285.803079	7999.847473	9.576282	-0.058124	4.815428
285.733580	8000.124097	9.581287	-0.058111	4.815509
285.816995	8000.073104	9.586291	-0.058126	4.815493
285.801487	7999.939287	9.591296	-0.058123	4.815454
285.650025	8000.167556	9.596301	-0.058095	4.815522
286.062692	7999.842057	9.601306	-0.058172	4.815425
286.053749	7999.973309	9.606311	-0.058170	4.815463
285.769031	7999.957931	9.611315	-0.058117	4.815460
285.874032	7999.892335	9.616320	-0.058136	4.815440
285.909649	7999.882223	9.621325	-0.058142	4.815437
285.878995	7999.868885	9.626330	-0.058137	4.815434
286.116010	7999.990291	9.631335	-0.058181	4.815468
286.080974	7999.844401	9.636339	-0.058174	4.815425
286.157630	7999.860605	9.641344	-0.058188	4.815430
286.100848	7999.969702	9.646349	-0.058177	4.815462
286.211439	7999.856120	9.651354	-0.058198	4.815428
286.191938	7999.897454	9.656359	-0.058194	4.815440
285.937399	7999.867615	9.661363	-0.058146	4.815433
286.085105	7999.943748	9.666368	-0.058174	4.815454
286.065234	7999.926314	9.671373	-0.058170	4.815449
286.128440	7999.960460	9.676378	-0.058182	4.815459
286.201982	7999.945629	9.681383	-0.058195	4.815454
286.103225	8000.101047	9.686387	-0.058177	4.815500
286.128857	7999.972178	9.691392	-0.058181	4.815463
286.126189	7999.949685	9.696397	-0.058181	4.815456
286.349933	7999.910614	9.701402	-0.058222	4.815444
286.365124	8000.032648	9.706407	-0.058225	4.815479
286.310751	7999.954816	9.711411	-0.058214	4.815457
286.182495	7999.922779	9.716416	-0.058190	4.815448
286.281382	8000.002384	9.721421	-0.058209	4.815471
286.363041	7999.928925	9.726426	-0.058224	4.815449
286.153388	7999.896619	9.731431	-0.058184	4.815440
286.368757	7999.937540	9.736435	-0.058224	4.815451
286.487672	7999.945892	9.741440	-0.058246	4.815453
286.322244	7999.950637	9.746445	-0.058216	4.815455
286.465597	7999.833320	9.751450	-0.058242	4.815420
286.560718	7999.963079	9.756455	-0.058260	4.815458
286.385679	8000.011470	9.761459	-0.058227	4.815473
286.458514	8000.019065	9.766464	-0.058240	4.815475
286.342029	7999.955169	9.771469	-0.058218	4.815457
286.427861	7999.969388	9.776474	-0.058234	4.815460
286.427978	8000.094380	9.781479	-0.058234	4.815497
286.394416	7999.923938	9.786483	-0.058228	4.815447
286.611135	7999.855905	9.791488	-0.058268	4.815426
286.330890	8000.037186	9.796493	-0.058216	4.815481
286.486279	7999.886946	9.801498	-0.058244	4.815436
286.492353	7999.956478	9.806503	-0.058245	4.815456
286.336749	7999.998779	9.811507	-0.058216	4.815469
286.316218	7999.945008	9.816512	-0.058212	4.815454
286.487763	7999.991620	9.821517	-0.058244	4.815467
286.697042	7999.893549	9.826522	-0.058283	4.815437
286.541599	7999.964700	9.831527	-0.058254	4.815459
286.558328	7999.954277	9.836531	-0.058257	4.815455
286.828151	7999.826218	9.841536	-0.058307	4.815417
286.538577	8000.143034	9.846541	-0.058253	4.815511
286.582535	7999.935404	9.851546	-0.058261	4.815450
286.659966	7999.865081	9.856551	-0.058275	4.815429
286.632408	7999.970386	9.861555	-0.058270	4.815460
286.730515	7999.928181	9.866560	-0.058288	4.815447
286.480370	8000.057605	9.871565	-0.058241	4.815486
286.575348	7999.801669	9.876570	-0.058259	4.815411
286.525957	7999.999566	9.881575	-0.058249	4.815469
286.641317	8000.028159	9.886579	-0.058271	4.815477
286.792271	7999.872504	9.891584	-0.058299	4.815430
286.628318	8000.129418	9.896589	-0.058268	4.815506
286.708615	7999.943753	9.901594	-0.058283	4.815452
286.837676	7999.957615	9.906599	-0.058307	4.815455
286.542977	7999.949550	9.911603	-0.058252	4.815454
286.706011	7999.837898	9.916608	-0.058282	4.815421
286.657054	7999.956741	9.921613	-0.058273	4.815456
286.689153	7999.918793	9.926618	-0.058278	4.815444
286.603898	8000.048791	9.931623	-0.058262	4.815483
286.632899	8000.140070	9.936627	-0.058268	4.815509
286.683653	7999.936825	9.941632	-0.058277	4.815450
286.846475	8000.095477	9.946637	-0.058307	4.815495
286.674830	7999.945200	9.951642	-0.058275	4.815452
286.854529	8000.012246	9.956647	-0.058308	4.815471
286.826088	8000.078007	9.961651	-0.058303	4.815490
286.605687	8000.025222	9.966656	-0.058262	4.815476
286.521285	8000.165919	9.971661	-0.058246	4.815518
286.726766	7999.940645	9.976666	-0.058284	4.815451
286.839211	8000.173259	9.981671	-0.058305	4.815518
286.779644	8000.164786	9.986675	-0.058294	4.815516
286.942416	7999.933467	9.991680	-0.058324	4.815448
286.812836	8000.115090	9.996685	-0.058299	4.815501
286.701466	7999.981830	10.001690	-0.058278	4.815463
286.899930	7999.972259	10.006695	-0.058315	4.815459
286.840550	8000.022553	10.011699	-0.058304	4.815474
286.926094	7999.872232	10.016704	-0.058320	4.815430
286.700592	7999.929410	10.021709	-0.058278	4.815448
286.979581	7999.944668	10.026714	-0.058329	4.815451
287.011250	7999.992186	10.031719	-0.058335	4.815464
286.846724	8000.023656	10.036723	-0.058304	4.815474
286.918511	7999.941487	10.041728	-0.058318	4.815450
286.882813	8000.081917	10.046733	-0.058311	4.815491
286.818870	7999.953711	10.051738	-0.058299	4.815454
286.874521	8000.050770	10.056743	-0.058309	4.815482
286.890052	8000.083064	10.061747	-0.058312	4.815492
286.935560	7999.911785	10.066752	-0.058320	4.815441
286.826312	7999.958053	10.071757	-0.058300	4.815455
287.000904	7999.980142	10.076762	-0.058332	4.815461
286.955404	7999.904592	10.081767	-0.058323	4.815439
286.775875	8000.180482	10.086771	-0.058290	4.815521
286.930817	7999.940487	10.091776	-0.058318	4.815450
286.874454	7999.982283	10.096781	-0.058308	4.815462
286.872299	8000.149975	10.101786	-0.058307	4.815511
287.045954	8000.042771	10.106791	-0.058339	4.815479
286.940558	8000.119019	10.111795	-0.058320	4.815502
286.904620	7999.968836	10.116800	-0.058313	4.815458
286.699694	8000.172725	10.121805	-0.058275	4.815519
286.875205	8000.006788	10.126810	-0.058307	4.815469
287.045650	8000.023467	10.131815	-0.058339	4.815473
286.738628	8000.123109	10.136819	-0.058281	4.815504
286.914584	7999.830039	10.141824	-0.058314	4.815418
286.876727	8000.033470	10.146829	-0.058307	4.815477
286.881547	7999.899984	10.151834	-0.058307	4.815438
286.938934	7999.957540	10.156839	-0.058318	4.815455
286.986276	8000.115363	10.161843	-0.058327	4.815501
287.145347	7999.945950	10.166848	-0.058356	4.815450
286.997669	8000.021502	10.171853	-0.058328	4.815473
287.099934	7999.936629	10.176858	-0.058347	4.815448
286.942956	7999.974634	10.181863	-0.058318	4.815460
286.761529	8000.051767	10.186867	-0.058284	4.815483
286.947044	7999.939416	10.191872	-0.058318	4.815449
287.018393	8000.019639	10.196877	-0.058332	4.815473
286.845944	8000.054184	10.201882	-0.058299	4.815483
287.005985	7999.959577	10.206887	-0.058329	4.815455
287.146857	8000.131759	10.211891	-0.058355	4.815505
287.036063	7999.976071	10.216896	-0.058334	4.815460
287.009276	7999.988438	10.221901	-0.058329	4.815464
287.084427	7999.985387	10.226906	-0.058343	4.815462
287.052221	7999.989117	10.231911	-0.058337	4.815464
286.889075	7999.955437	10.236915	-0.058306	4.815454
287.007099	7999.836634	10.241920	-0.058328	4.815419
286.920011	7999.966603	10.246925	-0.058312	4.815458
286.915053	7999.924840	10.251930	-0.058311	4.815445
286.930797	7999.963548	10.256935	-0.058313	4.815457
287.185701	8000.131196	10.261939	-0.058361	4.815504
287.255722	8000.067160	10.266944	-0.058374	4.815485
287.107220	8000.011283	10.271949	-0.058346	4.815470
287.109073	7999.992068	10.276954	-0.058346	4.815464
287.164543	7999.953436	10.281959	-0.058356	4.815453
286.899694	8000.114671	10.286963	-0.058307	4.815501
286.994553	8000.020060	10.291968	-0.058324	4.815473
287.057789	8000.000787	10.296973	-0.058336	4.815467
286.980535	7999.948219	10.301978	-0.058321	4.815452
287.061128	7999.842690	10.306983	-0.058336	4.815421
287.090597	8000.032270	10.311987	-0.058341	4.815476
287.260693	7999.901502	10.316992	-0.058373	4.815437
287.054136	8000.107502	10.321997	-0.058334	4.815498
287.054843	7999.876722	10.327002	-0.058334	4.815431
287.254160	7999.922723	10.332007	-0.058371	4.815443
287.200693	7999.975251	10.337011	-0.058361	4.815459
287.347575	7999.919959	10.342016	-0.058388	4.815442
287.312888	8000.018738	10.347021	-0.058382	4.815471
287.257733	7999.992175	10.352026	-0.058371	4.815464
287.196638	7999.933462	10.357031	-0.058360	4.815447
287.104569	8000.094334	10.362035	-0.058343	4.815494
287.421924	7999.874104	10.367040	-0.058401	4.815428
287.183744	8000.073173	10.372045	-0.058357	4.815488
287.003442	7999.888564	10.377050	-0.058323	4.815434
287.232531	8000.058991	10.382055	-0.058366	4.815483
287.218243	8000.055537	10.387059	-0.058363	4.815482
287.381296	7999.960979	10.392064	-0.058393	4.815454
287.386611	8000.120249	10.397069	-0.058394	4.815500
287.224966	7999.949834	10.402074	-0.058364	4.815451
287.236182	7999.957484	10.407079	-0.058366	4.815454
287.219102	7999.973216	10.412083	-0.058362	4.815458
287.257836	7999.828535	10.417088	-0.058369	4.815416
287.339257	8000.040339	10.422093	-0.058384	4.815477
287.395389	7999.827565	10.427098	-0.058395	4.815415
287.304798	7999.992735	10.432103	-0.058378	4.815464
287.243786	8000.052618	10.437107	-0.058366	4.815481
287.372083	7999.858125	10.442112	-0.058390	4.815424
287.227770	8000.020275	10.447117	-0.058363	4.815472
287.265710	7999.870238	10.452122	-0.058370	4.815428
287.305029	7999.947798	10.457127	-0.058377	4.815450
287.252150	8000.056962	10.462131	-0.058367	4.815483
287.372666	7999.832426	10.467136	-0.058389	4.815416
287.176984	7999.992662	10.472141	-0.058353	4.815464
287.283280	7999.953797	10.477146	-0.058372	4.815452
287.339076	7999.979275	10.482151	-0.058383	4.815459
287.159987	7999.822464	10.487155	-0.058349	4.815414
287.236041	7999.861096	10.492160	-0.058363	4.815425
287.472495	8000.015618	10.497165	-0.058407	4.815469
287.438278	7999.934910	10.502170	-0.058400	4.815446
287.395686	7999.889323	10.507175	-0.058392	4.815433
287.324929	7999.956524	10.512179	-0.058379	4.815453
287.499588	7999.944426	10.517184	-0.058411	4.815449
287.314003	7999.981960	10.522189	-0.058377	4.815460
287.228534	7999.970925	10.527194	-0.058361	4.815458
287.540052	7999.921546	10.532199	-0.058418	4.815442
287.434895	7999.989250	10.537203	-0.058399	4.815462
287.373340	7999.897409	10.542208	-0.058387	4.815435
287.416674	7999.942982	10.547213	-0.058395	4.815449
287.605214	7999.992012	10.552218	-0.058430	4.815462
287.536312	7999.865859	10.557223	-0.058417	4.815425
287.536324	7999.856230	10.562227	-0.058417	4.815423
287.666942	7999.754729	10.567232	-0.058441	4.815392
287.387220	7999.913583	10.572237	-0.058389	4.815440
287.387666	7999.884729	10.577242	-0.058389	4.815432
287.303100	7999.870504	10.582247	-0.058373	4.815428
287.613061	7999.943968	10.587251	-0.058430	4.815448
287.522114	7999.866600	10.592256	-0.058413	4.815426
287.469264	7999.952260	10.597261	-0.058403	4.815451
287.575478	7999.854630	10.602266	-0.058423	4.815422
287.672766	7999.859422	10.607271	-0.058441	4.815423
287.431643	7999.970832	10.612275	-0.058396	4.815457
287.592290	7999.762982	10.617280	-0.058425	4.815395
287.365194	7999.976123	10.622285	-0.058383	4.815459
287.463350	7999.830282	10.627290	-0.058401	4.815415
287.470679	7999.938299	10.632295	-0.058402	4.815447
287.349904	7999.894631	10.637299	-0.058380	4.815435
287.469388	7999.792947	10.642304	-0.058402	4.815404
287.405154	7999.905129	10.647309	-0.058390	4.815438
287.426995	7999.781539	10.652314	-0.058394	4.815401
287.425432	7999.930009	10.657319	-0.058393	4.815445
287.380355	7999.868355	10.662323	-0.058385	4.815427
287.698882	7999.777422	10.667328	-0.058444	4.815399
287.569969	7999.918457	10.672333	-0.058420	4.815441
287.417186	7999.903109	10.677338	-0.058391	4.815437
287.476717	7999.916896	10.682343	-0.058402	4.815441
287.392723	7999.903749	10.687347	-0.058386	4.815437
287.404197	7999.815245	10.692352	-0.058388	4.815411
287.309444	7999.904489	10.697357	-0.058370	4.815438
287.431466	7999.916098	10.702362	-0.058393	4.815441
287.695482	7999.927906	10.707367	-0.058442	4.815443
287.498673	7999.916108	10.712371	-0.058405	4.815440
287.411943	7999.861247	10.717376	-0.058389	4.815425
287.771963	7999.839376	10.722381	-0.058456	4.815417
287.632664	7999.886219	10.727386	-0.058430	4.815431
287.388315	7999.886461	10.732391	-0.058384	4.815432
287.415508	7999.910400	10.737395	-0.058389	4.815439
287.666474	7999.818356	10.742400	-0.058435	4.815411
287.420082	7999.968143	10.747405	-0.058390	4.815456
287.421411	7999.851693	10.752410	-0.058390	4.815422
287.590411	7999.869417	10.757415	-0.058421	4.815426
287.386926	7999.841484	10.762419	-0.058383	4.815419
287.634632	7999.797465	10.767424	-0.058429	4.815405
287.520767	7999.868232	10.772429	-0.058407	4.815426
287.289741	7999.939208	10.777434	-0.058364	4.815448
287.276018	7999.871659	10.782439	-0.058362	4.815429
287.279110	7999.880243	10.787443	-0.058362	4.815431
287.495691	7999.806866	10.792448	-0.058402	4.815409
287.300398	7999.945740	10.797453	-0.058366	4.815450
287.424890	7999.947774	10.802458	-0.058389	4.815450
287.486801	7999.887879	10.807463	-0.058400	4.815432
287.518754	7999.921512	10.812467	-0.058406	4.815442
287.606457	7999.730626	10.817472	-0.058422	4.815386
287.586287	7999.963196	10.822477	-0.058418	4.815454
287.499583	7999.855983	10.827482	-0.058402	4.815423
287.499890	7999.844222	10.832487	-0.058402	4.815419
287.713870	7999.855207	10.837491	-0.058441	4.815422
287.748192	7999.848279	10.842496	-0.058448	4.815419
287.485757	7999.896302	10.847501	-0.058399	4.815435
287.410602	7999.865137	10.852506	-0.058385	4.815426
287.590441	7999.900133	10.857511	-0.058418	4.815435
287.299230	7999.928451	10.862515	-0.058364	4.815445
287.401458	7999.929051	10.867520	-0.058382	4.815445
287.555664	8000.011706	10.872525	-0.058411	4.815468
287.502036	7999.818494	10.877530	-0.058401	4.815412
287.490738	7999.941163	10.882535	-0.058399	4.815448
287.585747	7999.930960	10.887539	-0.058416	4.815444
287.730167	7999.898064	10.892544	-0.058443	4.815434
287.297482	7999.815077	10.897549	-0.058362	4.815412
287.393786	7999.854042	10.902554	-0.058380	4.815423
287.554504	7999.842782	10.907559	-0.058410	4.815419
287.503765	7999.954118	10.912563	-0.058400	4.815452
287.544232	7999.845791	10.917568	-0.058407	4.815420
287.611300	7999.906712	10.922573	-0.058420	4.815437
287.641764	7999.969169	10.927578	-0.058425	4.815455
287.561112	7999.929365	10.932583	-0.058410	4.815444
287.554773	7999.945274	10.937587	-0.058409	4.815449
287.711007	7999.845262	10.942592	-0.058438	4.815419
287.705682	7999.863324	10.947597	-0.058437	4.815424
287.560463	7999.827801	10.952602	-0.058409	4.815414
287.667036	7999.874414	10.957607	-0.058429	4.815428
287.537130	7999.864785	10.962611	-0.058405	4.815425
287.567133	7999.849239	10.967616	-0.058410	4.815421
287.508464	7999.943350	10.972621	-0.058399	4.815449
287.756720	7999.817072	10.977626	-0.058445	4.815410
287.532125	7999.944781	10.982631	-0.058403	4.815449
287.501266	8000.094908	10.987635	-0.058397	4.815493
287.699048	7999.943226	10.992640	-0.058434	4.815448
287.683918	7999.978222	10.997645	-0.058431	4.815458
287.461310	8000.024762	11.002650	-0.058390	4.815473
287.886739	7999.982600	11.007655	-0.058469	4.815458
287.916379	7999.838836	11.012659	-0.058474	4.815416
287.971067	7999.851475	11.017664	-0.058484	4.815419
287.870247	7999.825229	11.022669	-0.058465	4.815412
287.944449	7999.973879	11.027674	-0.058479	4.815455
287.738202	7999.926668	11.032679	-0.058440	4.815443
287.660903	7999.931793	11.037683	-0.058426	4.815444
287.987664	7999.921128	11.042688	-0.058486	4.815440
287.729165	7999.944642	11.047693	-0.058438	4.815448
287.696749	8000.000722	11.052698	-0.058432	4.815464
287.735701	7999.868864	11.057703	-0.058439	4.815426
287.748811	7999.949199	11.062707	-0.058441	4.815449
287.680374	7999.952333	11.067712	-0.058428	4.815450
288.035574	7999.907946	11.072717	-0.058494	4.815436
287.936295	7999.875315	11.077722	-0.058476	4.815427
287.819717	7999.972748	11.082727	-0.058454	4.815456
287.773917	7999.848044	11.087731	-0.058445	4.815419
287.846195	7999.857767	11.092736	-0.058458	4.815422
287.935100	7999.862421	11.097741	-0.058475	4.815423
287.874096	7999.927647	11.102746	-0.058463	4.815442
288.017131	7999.931055	11.107751	-0.058490	4.815443
288.010088	7999.960841	11.112755	-0.058488	4.815451
287.888502	7999.894722	11.117760	-0.058465	4.815433
287.953965	7999.972712	11.122765	-0.058478	4.815455
287.963160	7999.854254	11.127770	-0.058479	4.815420
287.868204	7999.851611	11.132775	-0.058461	4.815420
287.622557	7999.848626	11.137779	-0.058415	4.815420
287.941879	7999.867754	11.142784	-0.058475	4.815424
287.887139	7999.939493	11.147789	-0.058464	4.815446
287.656072	7999.827768	11.152794	-0.058421	4.815414
287.970296	7999.888481	11.157799	-0.058479	4.815430
287.902971	7999.978177	11.162803	-0.058467	4.815457
287.940459	7999.830268	11.167808	-0.058474	4.815414
287.926407	7999.901608	11.172813	-0.058471	4.815434
287.967282	7999.863804	11.177818	-0.058478	4.815423
288.032187	7999.869132	11.182823	-0.058490	4.815424
288.004789	7999.921021	11.187827	-0.058485	4.815440
288.081947	7999.764149	11.192832	-0.058499	4.815394
287.964130	8000.005800	11.197837	-0.058477	4.815465
287.754926	7999.875202	11.202842	-0.058438	4.815428
288.000795	7999.869617	11.207847	-0.058484	4.815425
287.960781	7999.880698	11.212851	-0.058476	4.815428
287.917860	7999.801983	11.217856	-0.058468	4.815405
287.828717	7999.852856	11.222861	-0.058451	4.815421
288.023674	7999.849639	11.227866	-0.058487	4.815419
288.105427	7999.884092	11.232871	-0.058502	4.815429
288.017321	7999.998020	11.237875	-0.058486	4.815462
288.159701	7999.821920	11.242880	-0.058512	4.815410
288.215523	7999.982022	11.247885	-0.058522	4.815457
288.094677	7999.838987	11.252890	-0.058500	4.815415
288.113570	7999.943991	11.257895	-0.058503	4.815446
288.163131	7999.946930	11.262899	-0.058512	4.815447
288.082872	7999.787468	11.267904	-0.058497	4.815400
288.064153	7999.949548	11.272909	-0.058493	4.815448
288.066571	7999.836321	11.277914	-0.058494	4.815415
288.079202	7999.873910	11.282919	-0.058496	4.815426
287.906394	7999.936228	11.287923	-0.058464	4.815445
287.884520	7999.847176	11.292928	-0.058459	4.815419
287.919920	7999.936424	11.297933	-0.058466	4.815445
287.789034	7999.989816	11.302938	-0.058441	4.815461
287.951413	7999.855715	11.307943	-0.058471	4.815421
287.986480	7999.830636	11.312947	-0.058478	4.815414
288.062320	7999.922686	11.317952	-0.058492	4.815440
287.988820	7999.920395	11.322957	-0.058478	4.815440
287.876672	7999.994396	11.327962	-0.058457	4.815462
288.061704	7999.870283	11.332967	-0.058491	4.815425
287.868144	7999.993160	11.337971	-0.058455	4.815462
287.933868	7999.861743	11.342976	-0.058467	4.815423
287.973026	7999.880537	11.347981	-0.058474	4.815428
287.919689	7999.843319	11.352986	-0.058464	4.815418
288.062137	7999.894797	11.357991	-0.058491	4.815432
288.128135	7999.857405	11.362995	-0.058503	4.815421
288.279351	7999.851332	11.368000	-0.058531	4.815418
288.125090	7999.921434	11.373005	-0.058502	4.815439
288.039950	7999.823862	11.378010	-0.058486	4.815411
288.083382	7999.849137	11.383015	-0.058494	4.815419
287.882603	7999.991127	11.388019	-0.058456	4.815461
287.900491	7999.821528	11.393024	-0.058459	4.815411
288.139512	7999.841472	11.398029	-0.058504	4.815416
287.985389	7999.939356	11.403034	-0.058475	4.815445
287.948415	7999.890655	11.408039	-0.058468	4.815431
288.073935	7999.935444	11.413043	-0.058491	4.815444
288.140988	7999.836101	11.418048	-0.058503	4.815414
288.048368	7999.929654	11.423053	-0.058486	4.815442
288.055319	7999.943644	11.428058	-0.058487	4.815446
288.397289	7999.876603	11.433063	-0.058551	4.815425
288.082508	7999.909875	11.438067	-0.058492	4.815436
288.095442	7999.868406	11.443072	-0.058494	4.815424
288.182143	7999.851655	11.448077	-0.058510	4.815419
288.257220	7999.847534	11.453082	-0.058524	4.815417
288.219961	7999.894988	11.458087	-0.058517	4.815431
288.110107	7999.964752	11.463091	-0.058496	4.815452
288.153014	7999.855396	11.468096	-0.058504	4.815420
288.092691	7999.898196	11.473101	-0.058493	4.815433
287.973234	7999.919723	11.478106	-0.058470	4.815440
288.302809	7999.875983	11.483111	-0.058532	4.815425
288.238137	7999.836442	11.488115	-0.058519	4.815414
288.262778	7999.863545	11.493120	-0.058524	4.815422
288.153205	7999.875619	11.498125	-0.058503	4.815426
288.039260	7999.953863	11.503130	-0.058482	4.815449
288.064960	7999.858114	11.508135	-0.058486	4.815421
288.090136	7999.964289	11.513139	-0.058491	4.815452
288.314583	7999.731845	11.518144	-0.058533	4.815383
288.236794	7999.906843	11.523149	-0.058518	4.815435
288.136120	7999.883804	11.528154	-0.058499	4.815429
288.234205	7999.855488	11.533159	-0.058517	4.815420
288.209876	7999.883922	11.538163	-0.058513	4.815428
288.088387	7999.782547	11.543168	-0.058490	4.815399
288.068871	7999.917903	11.548173	-0.058486	4.815439
288.043858	8000.141850	11.553178	-0.058481	4.815504
288.197888	7999.885808	11.558183	-0.058510	4.815429
288.240511	7999.954876	11.563187	-0.058518	4.815449
288.427994	7999.848966	11.568192	-0.058552	4.815417
288.234108	7999.840421	11.573197	-0.058516	4.815415
288.146470	8000.082570	11.578202	-0.058500	4.815487
288.388465	7999.866439	11.583207	-0.058544	4.815422
288.320099	7999.819359	11.588211	-0.058531	4.815409
288.260180	7999.948708	11.593216	-0.058520	4.815447
288.347319	7999.904186	11.598221	-0.058536	4.815434
288.388201	7999.856765	11.603226	-0.058544	4.815419
288.377001	7999.899305	11.608231	-0.058542	4.815432
288.287846	7999.856156	11.613235	-0.058525	4.815420
288.159991	7999.829465	11.618240	-0.058501	4.815413
288.173850	7999.875622	11.623245	-0.058503	4.815426
288.100319	7999.829526	11.628250	-0.058489	4.815413
288.329950	7999.882437	11.633255	-0.058532	4.815427
288.355444	7999.845448	11.638259	-0.058537	4.815416
288.099674	7999.920291	11.643264	-0.058489	4.815439
288.251362	7999.974058	11.648269	-0.058517	4.815454
288.172124	7999.941756	11.653274	-0.058502	4.815445
288.295321	7999.872185	11.658279	-0.058525	4.815424
288.137119	7999.922990	11.663283	-0.058495	4.815440
288.278997	7999.822741	11.668288	-0.058521	4.815410
288.337495	7999.884591	11.673293	-0.058532	4.815428
288.219693	7999.882639	11.678298	-0.058510	4.815428
288.284990	7999.783268	11.683303	-0.058522	4.815399
288.158169	7999.947843	11.688307	-0.058498	4.815447
288.281130	7999.923142	11.693312	-0.058521	4.815439
288.218842	7999.950952	11.698317	-0.058509	4.815448
288.069954	7999.952762	11.703322	-0.058482	4.815449
287.982128	7999.956646	11.708327	-0.058465	4.815451
288.109363	8000.117924	11.713331	-0.058489	4.815497
288.187449	7999.942902	11.718336	-0.058503	4.815446
288.155953	7999.848349	11.723341	-0.058497	4.815418
288.067312	8000.100096	11.728346	-0.058480	4.815492
288.148357	7999.925124	11.733351	-0.058495	4.815441
288.254680	8000.088194	11.738355	-0.058515	4.815488
288.258650	7999.823274	11.743360	-0.058515	4.815410
288.380403	7999.971639	11.748365	-0.058538	4.815453
288.234554	7999.958541	11.753370	-0.058511	4.815450
288.354626	7999.950887	11.758375	-0.058533	4.815447
288.354335	7999.975443	11.763379	-0.058533	4.815454
288.197214	7999.852112	11.768384	-0.058503	4.815419
288.319730	7999.887235	11.773389	-0.058526	4.815429
288.264073	7999.936523	11.778394	-0.058515	4.815444
288.265316	7999.852123	11.783399	-0.058515	4.815419
288.287838	7999.893081	11.788403	-0.058519	4.815431
288.363491	7999.851575	11.793408	-0.058533	4.815418
288.082879	7999.838398	11.798413	-0.058481	4.815416
288.238856	7999.924288	11.803418	-0.058510	4.815440
288.471416	7999.836215	11.808423	-0.058553	4.815413
288.150985	7999.986922	11.813427	-0.058493	4.815459
288.244594	7999.920068	11.818432	-0.058511	4.815439
288.243847	7999.947822	11.823437	-0.058510	4.815447
288.039905	7999.930564	11.828442	-0.058472	4.815443
288.255078	7999.757799	11.833447	-0.058512	4.815391
288.281901	7999.969776	11.838451	-0.058517	4.815453
288.338718	7999.838212	11.843456	-0.058527	4.815414
288.350639	7999.914253	11.848461	-0.058529	4.815437
288.186322	7999.960685	11.853466	-0.058499	4.815451
288.415888	7999.904615	11.858471	-0.058541	4.815434
288.155462	7999.842623	11.863475	-0.058492	4.815417
288.072531	7999.855135	11.868480	-0.058477	4.815421
288.350368	7999.900292	11.873485	-0.058529	4.815433
288.294891	7999.943172	11.878490	-0.058518	4.815445
288.328974	7999.855039	11.883495	-0.058524	4.815419
288.303069	7999.877036	11.888499	-0.058519	4.815426
288.272925	7999.845543	11.893504	-0.058513	4.815417
288.196067	7999.836786	11.898509	-0.058499	4.815415
288.329597	7999.846448	11.903514	-0.058524	4.815417
288.402485	7999.876481	11.908519	-0.058537	4.815425
288.250929	7999.944491	11.913523	-0.058509	4.815446
288.250264	7999.933783	11.918528	-0.058509	4.815443
288.534911	7999.881825	11.923533	-0.058561	4.815426
288.203866	7999.891324	11.928538	-0.058500	4.815431
288.259887	7999.882616	11.933543	-0.058510	4.815428
288.403528	7999.877486	11.938547	-0.058536	4.815426
288.367040	7999.846956	11.943552	-0.058529	4.815417
288.431523	7999.920658	11.948557	-0.058541	4.815438
288.410105	7999.820927	11.953562	-0.058537	4.815409
288.537804	7999.887121	11.958567	-0.058561	4.815428
288.595617	7999.845321	11.963571	-0.058571	4.815415
288.416772	7999.813518	11.968576	-0.058538	4.815407
288.440642	7999.941041	11.973581	-0.058542	4.815444
288.455608	7999.857935	11.978586	-0.058545	4.815420
288.654229	7999.781057	11.983591	-0.058582	4.815396
288.537965	8000.028077	11.988595	-0.058560	4.815469
288.656576	7999.831285	11.993600	-0.058582	4.815411
288.517895	7999.821511	11.998605	-0.058556	4.815409
288.447415	7999.854528	12.003610	-0.058543	4.815419
288.579447	7999.887672	12.008615	-0.058567	4.815428
288.465630	7999.899675	12.013619	-0.058546	4.815432
288.522208	7999.776654	12.018624	-0.058556	4.815396
288.615387	7999.862580	12.023629	-0.058573	4.815420
288.620986	7999.873343	12.028634	-0.058574	4.815424
288.476040	7999.797223	12.033639	-0.058547	4.815402
288.352002	7999.892397	12.038643	-0.058524	4.815430
288.531683	7999.830165	12.043648	-0.058557	4.815411
288.526867	7999.889904	12.048653	-0.058556	4.815429
288.456016	7999.864151	12.053658	-0.058543	4.815422
288.444172	7999.828685	12.058663	-0.058540	4.815411
288.301419	7999.979109	12.063667	-0.058514	4.815456
288.403025	7999.865376	12.068672	-0.058532	4.815422
288.631807	7999.854168	12.073677	-0.058575	4.815418
288.541267	7999.922114	12.078682	-0.058558	4.815438
288.366733	7999.833754	12.083687	-0.058525	4.815413
288.403784	7999.915551	12.088691	-0.058532	4.815437
288.492703	7999.848621	12.093696	-0.058548	4.815417
288.378501	7999.895877	12.098701	-0.058527	4.815431
288.205228	7999.888739	12.103706	-0.058494	4.815430
288.546734	7999.849469	12.108711	-0.058558	4.815417
288.381788	7999.873453	12.113715	-0.058527	4.815425
288.421054	7999.853786	12.118720	-0.058534	4.815419
288.450163	7999.906604	12.123725	-0.058540	4.815434
288.321032	7999.855319	12.128730	-0.058515	4.815420
288.521154	7999.828681	12.133735	-0.058552	4.815411
288.501327	7999.955486	12.138739	-0.058549	4.815448
288.537805	7999.924019	12.143744	-0.058555	4.815439
288.526185	7999.959073	12.148749	-0.058553	4.815449
288.341131	7999.837419	12.153754	-0.058518	4.815414
288.769401	7999.784618	12.158759	-0.058598	4.815397
288.608980	7999.878125	12.163763	-0.058568	4.815425
288.604579	7999.841712	12.168768	-0.058567	4.815414
288.704315	7999.918131	12.173773	-0.058585	4.815436
288.580401	7999.843425	12.178778	-0.058562	4.815415
288.375568	7999.811194	12.183783	-0.058524	4.815407
288.242246	7999.916899	12.188787	-0.058499	4.815438
288.421537	7999.771323	12.193792	-0.058532	4.815395
288.523122	7999.918288	12.198797	-0.058551	4.815437
288.486622	7999.846088	12.203802	-0.058544	4.815416
288.527861	7999.839274	12.208807	-0.058551	4.815414
288.365355	7999.877188	12.213811	-0.058521	4.815426
288.240696	7999.790718	12.218816	-0.058498	4.815401
288.240824	7999.934945	12.223821	-0.058498	4.815444
288.340192	7999.891692	12.228826	-0.058516	4.815430
288.503466	7999.801411	12.233831	-0.058546	4.815403
288.507004	7999.877314	12.238835	-0.058547	4.815425
288.587903	7999.803841	12.243840	-0.058561	4.815404
288.444978	7999.951058	12.248845	-0.058535	4.815447
288.495262	7999.874944	12.253850	-0.058544	4.815425
288.721962	7999.807075	12.258855	-0.058586	4.815404
288.581611	7999.937239	12.263859	-0.058560	4.815443
288.390251	7999.843260	12.268864	-0.058524	4.815416
288.467285	7999.863746	12.273869	-0.058538	4.815422
288.424948	7999.827778	12.278874	-0.058530	4.815411
288.622888	7999.863073	12.283879	-0.058567	4.815421
288.434556	7999.966805	12.288883	-0.058532	4.815452
288.555788	7999.844848	12.293888	-0.058554	4.815416
288.542533	7999.838206	12.298893	-0.058551	4.815414
288.386632	7999.867680	12.303898	-0.058522	4.815423
288.620443	7999.774286	12.308903	-0.058566	4.815395
288.589479	7999.969287	12.313907	-0.058560	4.815452
288.582036	7999.821707	12.318912	-0.058558	4.815409
288.447318	7999.951963	12.323917	-0.058533	4.815448
288.423168	7999.816930	12.328922	-0.058528	4.815408
288.506464	7999.897351	12.333927	-0.058544	4.815431
288.525038	7999.861316	12.338931	-0.058547	4.815421
288.724621	7999.898776	12.343936	-0.058584	4.815431
288.523388	7999.900794	12.348941	-0.058546	4.815432
288.470367	7999.923414	12.353946	-0.058536	4.815439
288.697355	7999.840591	12.358951	-0.058578	4.815414
288.527690	7999.888003	12.363955	-0.058547	4.815429
288.337135	7999.833570	12.368960	-0.058511	4.815414
288.276228	7999.878497	12.373965	-0.058499	4.815427
288.444924	7999.855617	12.378970	-0.058531	4.815419
288.451317	7999.864256	12.383975	-0.058532	4.815422
288.369352	7999.937685	12.388979	-0.058516	4.815444
288.395418	7999.826983	12.393984	-0.058521	4.815411
288.410643	7999.976801	12.398989	-0.058524	4.815455
288.372040	7999.966536	12.403994	-0.058516	4.815452
288.433655	7999.796587	12.408999	-0.058528	4.815402
288.488707	7999.974840	12.414003	-0.058538	4.815454
288.677253	7999.887111	12.419008	-0.058573	4.815428
288.526023	7999.847214	12.424013	-0.058544	4.815417
288.455345	7999.959292	12.429018	-0.058531	4.815450
288.580375	7999.822439	12.434023	-0.058554	4.815409
288.452730	7999.892979	12.439027	-0.058530	4.815430
288.605226	7999.940349	12.444032	-0.058559	4.815444
288.511640	7999.965507	12.449037	-0.058541	4.815451
288.446800	7999.839420	12.454042	-0.058529	4.815415
288.517483	7999.877964	12.459047	-0.058542	4.815426
288.536199	7999.891080	12.464051	-0.058545	4.815429
288.637825	7999.839317	12.469056	-0.058564	4.815414
288.556399	7999.975792	12.474061	-0.058549	4.815454
288.560100	7999.832669	12.479066	-0.058549	4.815412
288.667665	7999.947680	12.484071	-0.058569	4.815445
288.563103	7999.890387	12.489075	-0.058549	4.815429
288.478862	7999.872961	12.494080	-0.058534	4.815424
288.703743	7999.898016	12.499085	-0.058575	4.815431
288.681525	7999.899774	12.504090	-0.058571	4.815431
288.549793	7999.887977	12.509095	-0.058546	4.815429
288.585874	7999.842615	12.514099	-0.058553	4.815415
288.794506	7999.936851	12.519104	-0.058592	4.815442
288.569334	7999.870095	12.524109	-0.058550	4.815423
288.530050	7999.829903	12.529114	-0.058542	4.815412
288.764995	7999.846576	12.534119	-0.058586	4.815415
288.602022	7999.950726	12.539123	-0.058555	4.815447
288.456154	7999.838263	12.544128	-0.058528	4.815414
288.720832	7999.870384	12.549133	-0.058577	4.815423
288.674644	7999.931580	12.554138	-0.058568	4.815441
288.650529	7999.839284	12.559143	-0.058564	4.815414
288.555375	7999.953096	12.564147	-0.058546	4.815448
288.755156	7999.926454	12.569152	-0.058583	4.815439
288.821068	7999.936072	12.574157	-0.058595	4.815441
288.636897	7999.943713	12.579162	-0.058560	4.815444
288.749234	7999.893194	12.584167	-0.058581	4.815429
288.626315	7999.938170	12.589171	-0.058558	4.815443
288.465134	7999.867125	12.594176	-0.058528	4.815423
288.734580	7999.884365	12.599181	-0.058578	4.815427
288.477302	7999.948499	12.604186	-0.058530	4.815447
288.569257	7999.920082	12.609191	-0.058547	4.815438
288.484237	7999.967818	12.614195	-0.058531	4.815452
288.495109	7999.849387	12.619200	-0.058533	4.815418
288.716293	7999.830575	12.624205	-0.058574	4.815411
288.561112	7999.924168	12.629210	-0.058545	4.815439
288.733124	7999.919506	12.634215	-0.058577	4.815437
288.504404	7999.930687	12.639219	-0.058534	4.815441
288.441626	7999.911478	12.644224	-0.058522	4.815436
288.491883	7999.947550	12.649229	-0.058531	4.815446
288.455672	7999.867876	12.654234	-0.058524	4.815423
288.490222	7999.780820	12.659239	-0.058531	4.815398
288.403751	7999.951402	12.664243	-0.058514	4.815448
288.587507	7999.870005	12.669248	-0.058548	4.815423
288.696707	7999.884609	12.674253	-0.058569	4.815427
288.401758	7999.918207	12.679258	-0.058514	4.815438
288.614525	7999.796687	12.684263	-0.058553	4.815402
288.610986	7999.985729	12.689267	-0.058552	4.815457
288.409974	7999.857401	12.694272	-0.058515	4.815420
288.638661	7999.850465	12.699277	-0.058557	4.815417
288.706112	8000.011828	12.704282	-0.058570	4.815464
288.613667	7999.890628	12.709287	-0.058552	4.815429
288.650466	7999.864509	12.714291	-0.058559	4.815421
288.473074	7999.956668	12.719296	-0.058526	4.815449
288.587199	7999.911521	12.724301	-0.058547	4.815435
288.453974	7999.989449	12.729306	-0.058522	4.815459
288.682440	7999.858571	12.734311	-0.058564	4.815419
288.618322	7999.885282	12.739315	-0.058552	4.815428
288.626050	7999.819152	12.744320	-0.058553	4.815408
288.621508	7999.905608	12.749325	-0.058552	4.815434
288.574893	7999.939017	12.754330	-0.058544	4.815444
288.450290	7999.844000	12.759335	-0.058520	4.815416
288.587072	7999.875085	12.764339	-0.058546	4.815425
288.578222	7999.927279	12.769344	-0.058544	4.815440
288.557713	7999.829700	12.774349	-0.058540	4.815412
288.531847	8000.020512	12.779354	-0.058535	4.815468
288.644643	7999.853541	12.784359	-0.058556	4.815418
288.552427	7999.958854	12.789363	-0.058538	4.815449
288.452487	7999.935828	12.794368	-0.058520	4.815443
288.682204	7999.934251	12.799373	-0.058562	4.815442
288.698727	7999.892841	12.804378	-0.058565	4.815429
288.576242	7999.776490	12.809383	-0.058542	4.815396
288.542719	7999.954353	12.814387	-0.058536	4.815448
288.606575	7999.832520	12.819392	-0.058547	4.815412
288.699605	7999.848995	12.824397	-0.058565	4.815417
288.420377	7999.949095	12.829402	-0.058513	4.815447
288.606060	7999.811103	12.834407	-0.058547	4.815406
288.643418	7999.984791	12.839411	-0.058554	4.815457
288.474730	8000.015124	12.844416	-0.058522	4.815466
288.540851	7999.882643	12.849421	-0.058534	4.815427
288.582194	7999.868352	12.854426	-0.058542	4.815423
288.704687	7999.939802	12.859431	-0.058565	4.815443
288.652492	7999.965641	12.864435	-0.058555	4.815451
288.766134	7999.804026	12.869440	-0.058576	4.815403
288.823480	7999.888294	12.874445	-0.058586	4.815428
288.656259	7999.948568	12.879450	-0.058555	4.815446
288.797269	7999.879289	12.884455	-0.058581	4.815425
288.606430	7999.906052	12.889459	-0.058545	4.815434
288.689912	7999.828348	12.894464	-0.058561	4.815411
288.683082	7999.894465	12.899469	-0.058559	4.815430
288.873949	7999.854854	12.904474	-0.058595	4.815418
288.951866	7999.795221	12.909479	-0.058609	4.815400
288.765398	7999.980186	12.914483	-0.058574	4.815455
288.715553	7999.828702	12.919488	-0.058565	4.815411
288.883401	7999.891283	12.924493	-0.058596	4.815428
288.600528	7999.835331	12.929498	-0.058543	4.815413
288.759675	7999.951190	12.934503	-0.058573	4.815446
288.764271	7999.881803	12.939507	-0.058573	4.815426
288.779686	7999.879907	12.944512	-0.058576	4.815425
288.770993	7999.827397	12.949517	-0.058574	4.815410
288.640893	7999.948114	12.954522	-0.058550	4.815446
288.675724	7999.825803	12.959527	-0.058556	4.815410
288.551166	7999.792756	12.964531	-0.058533	4.815401
288.622358	7999.835582	12.969536	-0.058546	4.815413
288.683760	7999.898548	12.974541	-0.058557	4.815431
288.548563	7999.843957	12.979546	-0.058532	4.815416
288.560441	7999.834523	12.984551	-0.058534	4.815413
288.473675	8000.067071	12.989555	-0.058518	4.815482
288.488416	7999.861091	12.994560	-0.058520	4.815421
288.627724	7999.874054	12.999565	-0.058546	4.815424
288.546406	7999.837444	13.004570	-0.058531	4.815414
288.696915	7999.876234	13.009575	-0.058559	4.815425
288.681197	7999.959300	13.014579	-0.058556	4.815449
288.646659	7999.940555	13.019584	-0.058549	4.815444
288.844966	7999.841234	13.024589	-0.058586	4.815414
288.702632	7999.969228	13.029594	-0.058559	4.815452
288.564459	7999.829113	13.034599	-0.058533	4.815412
288.532615	7999.990978	13.039603	-0.058527	4.815459
288.723448	7999.938546	13.044608	-0.058562	4.815443
288.706313	7999.955345	13.049613	-0.058559	4.815448
288.776158	7999.941523	13.054618	-0.058572	4.815444
288.742278	7999.734744	13.059623	-0.058565	4.815383
288.618630	7999.965615	13.064627	-0.058542	4.815451
288.690750	7999.945420	13.069632	-0.058556	4.815445
288.720248	7999.834774	13.074637	-0.058561	4.815413
288.681069	7999.951644	13.079642	-0.058553	4.815447
288.825148	7999.814035	13.084647	-0.058580	4.815406
288.802762	7999.983536	13.089651	-0.058576	4.815456
288.622211	7999.952772	13.094656	-0.058542	4.815448
288.569859	7999.956171	13.099661	-0.058532	4.815449
288.622590	7999.981600	13.104666	-0.058542	4.815456
288.971554	7999.877278	13.109671	-0.058607	4.815424
288.891370	7999.950737	13.114675	-0.058592	4.815446
288.763882	7999.946489	13.119680	-0.058568	4.815445
288.891502	7999.818225	13.124685	-0.058591	4.815407
288.791921	7999.961881	13.129690	-0.058573	4.815449
288.644063	7999.826949	13.134695	-0.058545	4.815411
288.671480	7999.981242	13.139699	-0.058550	4.815456
288.746909	7999.839298	13.144704	-0.058564	4.815414
288.685115	7999.853226	13.149709	-0.058552	4.815418
288.622696	7999.948345	13.154714	-0.058540	4.815446
288.656756	7999.956371	13.159719	-0.058547	4.815449
288.713267	7999.882497	13.164723	-0.058557	4.815427
288.709259	7999.973235	13.169728	-0.058556	4.815453
288.843062	7999.957260	13.174733	-0.058581	4.815448
288.730072	7999.979961	13.179738	-0.058560	4.815455
288.488556	7999.852036	13.184743	-0.058514	4.815419
288.587113	7999.876080	13.189747	-0.058533	4.815425
288.642456	7999.918647	13.194752	-0.058543	4.815438
288.619546	7999.998389	13.199757	-0.058538	4.815461
288.672516	7999.985358	13.204762	-0.058548	4.815457
288.877125	7999.874387	13.209767	-0.058586	4.815424
288.886549	7999.840339	13.214771	-0.058588	4.815414
288.856872	7999.914628	13.219776	-0.058582	4.815435
288.942286	7999.854050	13.224781	-0.058598	4.815417
288.769724	7999.987959	13.229786	-0.058565	4.815457
288.757955	7999.833896	13.234791	-0.058563	4.815412
288.770885	7999.972993	13.239795	-0.058565	4.815453
288.625748	7999.913964	13.244800	-0.058538	4.815436
288.776863	7999.794635	13.249805	-0.058566	4.815401
288.720581	7999.917634	13.254810	-0.058556	4.815437
288.909947	7999.857698	13.259815	-0.058591	4.815419
288.879305	7999.908466	13.264819	-0.058585	4.815434
288.605059	7999.843039	13.269824	-0.058533	4.815416
288.770020	7999.794455	13.274829	-0.058564	4.815401
288.899433	7999.872430	13.279834	-0.058588	4.815423
288.670900	7999.785318	13.284839	-0.058545	4.815399
288.669632	7999.916702	13.289843	-0.058545	4.815437
288.738706	7999.778928	13.294848	-0.058558	4.815396
288.771640	7999.891642	13.299853	-0.058564	4.815429
288.738112	7999.876119	13.304858	-0.058557	4.815425
288.893991	7999.892560	13.309863	-0.058586	4.815429
288.898636	7999.876596	13.314867	-0.058587	4.815424
288.752642	7999.942561	13.319872	-0.058560	4.815444
288.719107	7999.869342	13.324877	-0.058553	4.815423
288.677997	7999.931690	13.329882	-0.058545	4.815441
288.635551	7999.814519	13.334887	-0.058537	4.815407
288.812534	7999.939219	13.339891	-0.058570	4.815443
288.865194	7999.932593	13.344896	-0.058580	4.815441
288.885755	7999.845305	13.349901	-0.058583	4.815415
288.635030	7999.945874	13.354906	-0.058537	4.815446
288.797323	7999.858782	13.359911	-0.058567	4.815419
288.652526	7999.896987	13.364915	-0.058539	4.815431
288.576915	7999.951288	13.369920	-0.058525	4.815448
288.760308	7999.838901	13.374925	-0.058559	4.815414
288.730624	7999.960201	13.379930	-0.058554	4.815449
288.822564	7999.853788	13.384935	-0.058571	4.815418
288.798206	7999.860853	13.389939	-0.058566	4.815420
288.709190	7999.957671	13.394944	-0.058549	4.815449
288.805097	7999.915430	13.399949	-0.058567	4.815436
288.625114	7999.969082	13.404954	-0.058533	4.815453
288.811942	7999.900557	13.409959	-0.058568	4.815432
288.935383	7999.978435	13.414963	-0.058591	4.815454
288.915571	7999.936426	13.419968	-0.058587	4.815442
288.935892	7999.865161	13.424973	-0.058590	4.815421
288.855050	7999.962114	13.429978	-0.058575	4.815449
288.832049	7999.820688	13.434983	-0.058571	4.815408
288.704711	7999.975640	13.439987	-0.058547	4.815454
288.744994	7999.889746	13.444992	-0.058554	4.815429
288.920397	7999.799664	13.449997	-0.058587	4.815402
288.881152	7999.853495	13.455002	-0.058579	4.815418
288.890168	7999.898505	13.460007	-0.058581	4.815431
288.954365	7999.926259	13.465011	-0.058593	4.815439
288.627437	7999.837528	13.470016	-0.058532	4.815414
288.891460	7999.877117	13.475021	-0.058581	4.815424
288.748059	7999.868333	13.480026	-0.058554	4.815423
288.723862	7999.956602	13.485031	-0.058549	4.815449
288.750347	7999.875823	13.490035	-0.058554	4.815425
288.891579	7999.923008	13.495040	-0.058580	4.815438
289.026373	7999.938034	13.500045	-0.058605	4.815442
288.921059	7999.990778	13.505050	-0.058585	4.815458
289.040011	7999.951053	13.510055	-0.058607	4.815445
289.021569	7999.839618	13.515059	-0.058604	4.815413
288.983495	7999.947959	13.520064	-0.058596	4.815445
288.931326	7999.846654	13.525069	-0.058586	4.815415
288.979009	7999.982049	13.530074	-0.058595	4.815455
289.002440	7999.808264	13.535079	-0.058599	4.815404
288.800071	7999.992967	13.540083	-0.058562	4.815459
288.852217	7999.803629	13.545088	-0.058571	4.815403
289.060359	7999.940596	13.550093	-0.058610	4.815442
288.988873	7999.954364	13.555098	-0.058596	4.815447
289.003480	7999.943907	13.560103	-0.058599	4.815444
289.057693	7999.912732	13.565107	-0.058609	4.815434
288.960360	7999.848079	13.570112	-0.058591	4.815416
288.821884	7999.801981	13.575117	-0.058565	4.815403
288.792814	7999.964961	13.580122	-0.058559	4.815451
288.808630	7999.886143	13.585127	-0.058562	4.815428
288.959984	7999.825582	13.590131	-0.058590	4.815409
288.867694	7999.937305	13.595136	-0.058573	4.815442
288.956060	7999.826559	13.600141	-0.058589	4.815409
288.832217	7999.948447	13.605146	-0.058566	4.815446
288.773009	7999.844889	13.610151	-0.058554	4.815416
288.892684	7999.943004	13.615155	-0.058577	4.815444
288.775398	7999.950677	13.620160	-0.058555	4.815447
288.869205	7999.849637	13.625165	-0.058572	4.815417
288.711257	7999.865188	13.630170	-0.058542	4.815422
288.665896	7999.877250	13.635175	-0.058534	4.815426
288.696925	7999.853173	13.640179	-0.058539	4.815419
288.896194	7999.957940	13.645184	-0.058576	4.815448
289.116760	7999.763893	13.650189	-0.058617	4.815390
288.898777	7999.895986	13.655194	-0.058577	4.815430
288.826646	7999.876622	13.660199	-0.058563	4.815425
289.065906	7999.895503	13.665203	-0.058607	4.815429
288.948219	7999.845474	13.670208	-0.058585	4.815415
288.843867	7999.885412	13.675213	-0.058566	4.815427
288.517358	7999.946270	13.680218	-0.058505	4.815447
288.934378	7999.784305	13.685223	-0.058582	4.815397
288.895379	7999.939642	13.690227	-0.058575	4.815443
289.012516	7999.812274	13.695232	-0.058596	4.815405
288.922576	7999.986006	13.700237	-0.058580	4.815456
289.019089	7999.927747	13.705242	-0.058597	4.815439
288.895224	7999.943859	13.710247	-0.058574	4.815444
288.948920	7999.850706	13.715251	-0.058584	4.815417
288.956814	7999.946983	13.720256	-0.058585	4.815445
289.002651	7999.868659	13.725261	-0.058594	4.815422
288.937373	7999.837655	13.730266	-0.058581	4.815413
289.169796	7999.931215	13.735271	-0.058625	4.815439
289.110161	7999.874661	13.740275	-0.058613	4.815423
288.995767	7999.826822	13.745280	-0.058592	4.815409
289.108470	7999.866059	13.750285	-0.058613	4.815420
288.953842	7999.936155	13.755290	-0.058584	4.815442
288.972918	7999.914018	13.760295	-0.058587	4.815435
288.928473	7999.888700	13.765299	-0.058579	4.815428
288.932860	7999.924017	13.770304	-0.058579	4.815438
288.861272	7999.846966	13.775309	-0.058566	4.815416
288.781384	7999.970646	13.780314	-0.058551	4.815453
288.967015	7999.862569	13.785319	-0.058585	4.815420
288.906085	7999.891469	13.790323	-0.058574	4.815429
288.784652	7999.826420	13.795328	-0.058551	4.815410
289.026723	7999.925481	13.800333	-0.058596	4.815438
289.011615	7999.939109	13.805338	-0.058593	4.815442
289.093069	7999.834659	13.810343	-0.058608	4.815411
289.132282	7999.874823	13.815347	-0.058615	4.815423
289.238376	7999.833818	13.820352	-0.058635	4.815410
289.203023	7999.905877	13.825357	-0.058628	4.815432
289.031449	7999.899835	13.830362	-0.058596	4.815431
289.033201	7999.842155	13.835367	-0.058596	4.815414
289.058982	7999.745337	13.840371	-0.058601	4.815385
289.176240	7999.912862	13.845376	-0.058622	4.815434
289.012918	7999.824686	13.850381	-0.058592	4.815409
288.885801	7999.961478	13.855386	-0.058568	4.815449
289.069336	7999.913199	13.860391	-0.058602	4.815434
288.917773	7999.841243	13.865395	-0.058574	4.815414
288.899002	7999.921054	13.870400	-0.058570	4.815438
288.918051	7999.846563	13.875405	-0.058573	4.815416
288.823568	7999.963592	13.880410	-0.058556	4.815450
288.983552	7999.840135	13.885415	-0.058585	4.815414
288.944864	8000.018984	13.890419	-0.058578	4.815466
288.865735	7999.925782	13.895424	-0.058563	4.815439
288.981585	7999.821899	13.900429	-0.058584	4.815408
288.884197	7999.967728	13.905434	-0.058566	4.815451
288.930438	7999.841331	13.910439	-0.058575	4.815414
289.087818	7999.900534	13.915443	-0.058604	4.815431
288.890789	7999.847062	13.920448	-0.058567	4.815416
289.062401	7999.881926	13.925453	-0.058599	4.815425
288.945152	7999.863957	13.930458	-0.058577	4.815421
288.941668	7999.812601	13.935463	-0.058576	4.815406
288.989441	7999.914875	13.940467	-0.058585	4.815435
288.933395	7999.873339	13.945472	-0.058574	4.815424
289.085169	7999.872617	13.950477	-0.058602	4.815423
289.030066	7999.883450	13.955482	-0.058592	4.815426
288.991827	7999.904176	13.960487	-0.058585	4.815432
288.968935	7999.881349	13.965491	-0.058580	4.815426
289.071231	7999.944988	13.970496	-0.058599	4.815444
289.094976	7999.853479	13.975501	-0.058603	4.815417
288.857727	7999.861315	13.980506	-0.058559	4.815420
289.080876	7999.932285	13.985511	-0.058600	4.815440
289.055585	7999.883776	13.990515	-0.058596	4.815426
289.031253	7999.958153	13.995520	-0.058591	4.815448
289.073700	7999.972728	14.000525	-0.058599	4.815452
289.175651	7999.910285	14.005530	-0.058617	4.815433
288.955407	7999.902374	14.010535	-0.058576	4.815432
289.137880	7999.895747	14.015539	-0.058610	4.815429
289.051338	7999.966964	14.020544	-0.058594	4.815450
289.120456	7999.764015	14.025549	-0.058606	4.815391
288.917364	7999.967938	14.030554	-0.058569	4.815451
288.984859	7999.966898	14.035559	-0.058581	4.815451
289.185736	7999.821676	14.040563	-0.058618	4.815407
289.089771	7999.913039	14.045568	-0.058600	4.815434
289.091040	7999.933347	14.050573	-0.058600	4.815440
289.028808	7999.877818	14.055578	-0.058589	4.815424
288.974446	7999.931401	14.060583	-0.058578	4.815440
289.190440	7999.868698	14.065587	-0.058618	4.815421
288.993485	7999.958399	14.070592	-0.058582	4.815448
289.300815	7999.840571	14.075597	-0.058639	4.815412
289.143380	7999.836899	14.080602	-0.058609	4.815412
289.127273	7999.769308	14.085607	-0.058606	4.815392
289.229483	7999.977187	14.090611	-0.058625	4.815453
289.029463	7999.849942	14.095616	-0.058587	4.815416
289.057521	7999.843980	14.100621	-0.058593	4.815414
289.127601	7999.852599	14.105626	-0.058605	4.815417
289.076956	7999.839999	14.110631	-0.058596	4.815413
289.022213	7999.927766	14.115635	-0.058586	4.815439
289.062897	7999.832262	14.120640	-0.058593	4.815411
289.201535	7999.901841	14.125645	-0.058619	4.815431
289.053980	7999.852388	14.130650	-0.058591	4.815417
289.128600	7999.843987	14.135655	-0.058605	4.815414
289.246704	7999.934598	14.140659	-0.058627	4.815440
289.176605	7999.768890	14.145664	-0.058613	4.815392
289.324973	7999.902737	14.150669	-0.058641	4.815430
289.377697	7999.862990	14.155674	-0.058650	4.815419
289.445697	7999.867301	14.160679	-0.058663	4.815419
289.225947	7999.793154	14.165683	-0.058622	4.815399
289.265505	7999.981839	14.170688	-0.058629	4.815454
289.442408	7999.755019	14.175693	-0.058662	4.815387
289.078416	7999.978733	14.180698	-0.058594	4.815454
289.022932	8000.016271	14.185703	-0.058584	4.815465
289.224378	7999.970423	14.190707	-0.058621	4.815451
289.376331	7999.858586	14.195712	-0.058649	4.815417
289.296079	7999.816651	14.200717	-0.058634	4.815405
289.148401	7999.884725	14.205722	-0.058606	4.815426
289.244735	7999.817917	14.210727	-0.058624	4.815406
289.168278	7999.889299	14.215731	-0.058610	4.815427
289.192896	7999.833063	14.220736	-0.058614	4.815411
289.387236	7999.804194	14.225741	-0.058650	4.815401
289.308171	7999.902245	14.230746	-0.058635	4.815430
289.171832	7999.836950	14.235751	-0.058610	4.815412
289.000509	7999.849076	14.240755	-0.058578	4.815416
289.123739	7999.934429	14.245760	-0.058600	4.815441
288.966293	7999.829255	14.250765	-0.058571	4.815411
289.216971	7999.856871	14.255770	-0.058617	4.815418
289.328372	7999.886471	14.260775	-0.058638	4.815426
289.040300	7999.833637	14.265779	-0.058584	4.815412
288.885983	7999.942203	14.270784	-0.058555	4.815444
289.288543	7999.824873	14.275789	-0.058630	4.815408
289.225958	7999.533216	14.280794	-0.058618	4.815323
289.016591	7996.372885	14.285799	-0.058577	4.814400
289.221955	7990.791467	14.290803	-0.058611	4.812768
289.150370	7983.916888	14.295808	-0.058593	4.810758
288.926052	7976.697095	14.300813	-0.058547	4.808647
288.836243	7969.033698	14.305818	-0.058525	4.806404
288.912152	7961.216601	14.310823	-0.058534	4.804115
288.960085	7953.368690	14.315827	-0.058538	4.801816
288.707554	7945.354922	14.320832	-0.058485	4.799468
288.918284	7937.446830	14.325837	-0.058519	4.797148
288.844353	7929.401058	14.330842	-0.058500	4.794788
288.855554	7921.419006	14.335847	-0.058497	4.792445
288.725062	7913.358056	14.340851	-0.058467	4.790078
288.724611	7905.381599	14.345856	-0.058462	4.787734
288.894826	7897.357292	14.350861	-0.058488	4.785375
288.685810	7889.440968	14.355866	-0.058444	4.783047
288.763914	7881.408383	14.360871	-0.058453	4.780683
288.538238	7873.491243	14.365875	-0.058405	4.778353
288.461118	7865.406235	14.370880	-0.058386	4.775972
288.463480	7857.419535	14.375885	-0.058381	4.773618
288.479207	7849.334269	14.380890	-0.058378	4.771234
288.412241	7841.319720	14.385895	-0.058360	4.768870
288.257145	7833.402207	14.390899	-0.058326	4.766534
288.336092	7825.316039	14.395904	-0.058335	4.764146
288.407667	7817.404968	14.400909	-0.058343	4.761809
288.381021	7809.382554	14.405914	-0.058333	4.759438
288.193048	7801.397108	14.410919	-0.058293	4.757077
288.271174	7793.380778	14.415923	-0.058302	4.754705
288.074317	7785.306287	14.420928	-0.058260	4.752315
288.083328	7777.268780	14.425933	-0.058256	4.749935
287.894523	7769.303731	14.430938	-0.058216	4.747575
288.009933	7761.316492	14.435943	-0.058232	4.745207
287.913413	7753.377283	14.440947	-0.058209	4.742852
288.023955	7745.321140	14.445952	-0.058224	4.740461
287.995252	7737.332797	14.450957	-0.058213	4.738089
287.837939	7729.299921	14.455962	-0.058178	4.735703
287.947585	7721.305257	14.460967	-0.058193	4.733327
287.935894	7713.276685	14.465971	-0.058186	4.730939
287.806589	7705.258426	14.470976	-0.058156	4.728554
287.870002	7697.276439	14.475981	-0.058163	4.726178
287.850725	7689.334392	14.480986	-0.058154	4.723813
287.825332	7681.313534	14.485991	-0.058144	4.721423
287.700708	7673.319987	14.490995	-0.058115	4.719040
287.718806	7665.328588	14.496000	-0.058113	4.716656
287.851725	7657.360993	14.501005	-0.058133	4.714278
287.679610	7649.268456	14.506010	-0.058095	4.711863
287.764605	7641.265730	14.511015	-0.058106	4.709472
287.814492	7633.308551	14.516019	-0.058110	4.707093
287.505954	7625.248358	14.521024	-0.058047	4.704684
287.358386	7617.328157	14.526029	-0.058014	4.702315
287.344269	7609.281566	14.531034	-0.058006	4.699906
287.239759	7601.319789	14.536039	-0.057981	4.697522
287.370689	7593.277203	14.541043	-0.058000	4.695112
287.282909	7585.281028	14.546048	-0.057978	4.692714
287.489980	7577.273127	14.551053	-0.058012	4.690312
287.391768	7569.330859	14.556058	-0.057988	4.687929
287.381515	7561.280924	14.561063	-0.057981	4.685512
287.264700	7553.316633	14.566067	-0.057954	4.683119
287.327506	7545.276446	14.571072	-0.057960	4.680703
287.178544	7537.320240	14.576077	-0.057927	4.678310
287.141013	7529.294043	14.581082	-0.057914	4.675895
287.221926	7521.200016	14.586087	-0.057924	4.673459
287.085395	7513.150623	14.591091	-0.057893	4.671034
286.855802	7505.184806	14.596096	-0.057845	4.668634
287.016974	7497.184482	14.601101	-0.057870	4.666222
286.821503	7489.200235	14.606106	-0.057828	4.663813
286.802554	7481.246737	14.611111	-0.057819	4.661413
286.915402	7473.243060	14.616115	-0.057835	4.658996
286.872755	7465.226427	14.621120	-0.057821	4.656574
286.996414	7457.247583	14.626125	-0.057839	4.654162
286.922408	7449.230939	14.631130	-0.057820	4.651737
286.755708	7441.178016	14.636135	-0.057784	4.649301
286.795197	7433.235102	14.641139	-0.057786	4.646896
286.835920	7425.178836	14.646144	-0.057788	4.644455
286.833814	7417.293528	14.651149	-0.057782	4.642065
286.647193	7409.198831	14.656154	-0.057742	4.639611
286.697382	7401.237554	14.661159	-0.057746	4.637195
286.606026	7393.185571	14.666163	-0.057724	4.634751
286.289719	7385.211517	14.671168	-0.057659	4.632329
286.534596	7377.188100	14.676173	-0.057699	4.629891
286.633634	7369.177891	14.681178	-0.057713	4.627456
286.454054	7361.174671	14.686183	-0.057674	4.625021
286.382894	7353.205569	14.691187	-0.057655	4.622596
286.489429	7345.163923	14.696192	-0.057670	4.620147
286.484819	7337.238122	14.701197	-0.057663	4.617732
286.129168	7329.157704	14.706202	-0.057592	4.615268
286.083385	7321.168734	14.711207	-0.057578	4.612832
286.321730	7313.177826	14.716211	-0.057617	4.610393
286.181296	7305.143157	14.721216	-0.057585	4.607940
286.177372	7297.148512	14.726221	-0.057579	4.605498
286.038394	7289.176601	14.731226	-0.057548	4.603061
286.095750	7281.129182	14.736231	-0.057553	4.600600
285.922996	7273.196482	14.741235	-0.057516	4.598172
285.932588	7265.135269	14.746240	-0.057512	4.595704
286.042914	7257.133261	14.751245	-0.057527	4.593253
285.883415	7249.096237	14.756250	-0.057492	4.590790
286.005830	7241.121074	14.761255	-0.057510	4.588345
285.783557	7233.122368	14.766259	-0.057463	4.585890
285.717159	7225.095143	14.771264	-0.057445	4.583426
285.681416	7217.127068	14.776269	-0.057433	4.580979
285.766667	7209.171073	14.781274	-0.057444	4.578534
285.899384	7201.149124	14.786279	-0.057463	4.576068
285.522297	7193.145200	14.791283	-0.057388	4.573605
285.570870	7185.084524	14.796288	-0.057391	4.571124
285.783017	7177.115817	14.801293	-0.057425	4.568670
285.600805	7169.078819	14.806298	-0.057386	4.566193
285.492226	7161.126967	14.811303	-0.057360	4.563742
285.564087	7153.171625	14.816307	-0.057369	4.561288
285.338762	7145.116633	14.821312	-0.057321	4.558801
285.249575	7137.185804	14.826317	-0.057299	4.556352
285.243562	7129.099291	14.831322	-0.057293	4.553854
285.363320	7121.044889	14.836327	-0.057310	4.551364
285.440954	7113.086893	14.841331	-0.057319	4.548903
285.266104	7105.071970	14.846336	-0.057281	4.546422
285.361346	7097.098342	14.851341	-0.057293	4.543953
285.050565	7089.162520	14.856346	-0.057230	4.541494
285.070681	7081.073148	14.861351	-0.057228	4.538986
285.217778	7073.149502	14.866355	-0.057250	4.536529
285.315233	7065.052388	14.871360	-0.057263	4.534016
285.082631	7057.100553	14.876365	-0.057214	4.531547
284.909538	7049.055312	14.881370	-0.057177	4.529047
284.934923	7041.092569	14.886375	-0.057176	4.526572
285.069196	7033.090272	14.891379	-0.057196	4.524083
285.017464	7025.131776	14.896384	-0.057181	4.521607
285.160818	7017.095041	14.901389	-0.057202	4.519105
285.084984	7009.136495	14.906394	-0.057183	4.516625
284.880451	7001.084222	14.911399	-0.057139	4.514115
285.041952	6993.019606	14.916403	-0.057164	4.511600
284.892549	6985.009966	14.921408	-0.057131	4.509100
284.769500	6977.075590	14.926413	-0.057102	4.506622
284.784975	6969.017572	14.931418	-0.057100	4.504105
284.530631	6961.072252	14.936423	-0.057047	4.501621
284.648571	6953.043288	14.941427	-0.057064	4.499110
284.491719	6945.066148	14.946432	-0.057029	4.496614
284.651256	6937.053690	14.951437	-0.057054	4.494105
284.533859	6929.061226	14.956442	-0.057026	4.491601
284.358172	6921.045956	14.961447	-0.056988	4.489088
284.415760	6913.081716	14.966451	-0.056994	4.486591
284.472528	6905.007523	14.971456	-0.056999	4.484057
284.510441	6897.073266	14.976461	-0.057001	4.481566
284.446116	6889.074935	14.981466	-0.056983	4.479053
284.298453	6881.077048	14.986471	-0.056950	4.476539
284.291281	6873.082200	14.991475	-0.056944	4.474024
284.186267	6865.002680	14.996480	-0.056919	4.471482
284.127338	6856.989740	15.001485	-0.056902	4.468958
284.198208	6848.995726	15.006490	-0.056910	4.466440
284.082263	6840.992527	15.011495	-0.056883	4.463917
284.275981	6833.034785	15.016499	-0.056914	4.461408
284.301071	6825.029079	15.021504	-0.056913	4.458881
284.180850	6817.027701	15.026509	-0.056886	4.456354
284.013346	6808.994951	15.031514	-0.056849	4.453816
284.017509	6800.995304	15.036519	-0.056844	4.451287
284.047017	6793.029490	15.041523	-0.056844	4.448768
283.793661	6784.996899	15.046528	-0.056792	4.446225
284.092288	6777.043562	15.051533	-0.056842	4.443707
283.997744	6769.033867	15.056538	-0.056819	4.441169
283.777366	6761.017703	15.061543	-0.056773	4.438627
283.678366	6753.031127	15.066547	-0.056749	4.436093
283.552307	6744.961035	15.071552	-0.056720	4.433531
283.523554	6736.934587	15.076557	-0.056709	4.430982
283.528455	6728.963372	15.081562	-0.056705	4.428449
283.523274	6720.931098	15.086567	-0.056699	4.425895
283.537878	6713.002272	15.091571	-0.056696	4.423373
283.339628	6704.943866	15.096576	-0.056654	4.420807
283.373127	6696.975905	15.101581	-0.056655	4.418269
283.373211	6688.973852	15.106586	-0.056649	4.415719
283.276459	6680.966182	15.111591	-0.056626	4.413166
283.219002	6672.974318	15.116595	-0.056610	4.410616
283.238235	6665.032820	15.121600	-0.056608	4.408081
283.404810	6656.955749	15.126605	-0.056634	4.405501
283.182492	6648.992210	15.131610	-0.056587	4.402955
283.248784	6640.973972	15.136615	-0.056594	4.400391
283.245208	6633.022028	15.141619	-0.056588	4.397847
283.081741	6624.958454	15.146624	-0.056552	4.395264
283.263530	6616.943504	15.151629	-0.056581	4.392698
283.284629	6608.902834	15.156634	-0.056579	4.390121
283.118782	6600.965510	15.161639	-0.056543	4.387574
283.116806	6592.953149	15.166643	-0.056537	4.385003
282.990251	6584.987567	15.171648	-0.056508	4.382444
282.942998	6576.962125	15.176653	-0.056494	4.379865
282.703516	6569.014835	15.181658	-0.056444	4.377309
282.762241	6560.942614	15.186663	-0.056450	4.374713
282.895486	6553.009543	15.191667	-0.056469	4.372160
282.806294	6544.907885	15.196672	-0.056447	4.369551
282.595685	6536.967412	15.201677	-0.056403	4.366991
282.673193	6528.955506	15.206682	-0.056412	4.364408
282.812540	6521.008071	15.211687	-0.056432	4.361845
282.707236	6512.988826	15.216691	-0.056407	4.359255
282.646065	6505.002514	15.221696	-0.056390	4.356675
282.796819	6496.947212	15.226701	-0.056413	4.354073
282.627495	6488.865477	15.231706	-0.056376	4.351458
282.467412	6480.860828	15.236711	-0.056341	4.348867
282.655648	6472.897254	15.241715	-0.056371	4.346290
282.456559	6464.929015	15.246720	-0.056328	4.343707
282.536932	6456.952062	15.251725	-0.056338	4.341121
282.596594	6448.963915	15.256730	-0.056344	4.338531
282.441443	6440.994713	15.261735	-0.056309	4.335943
282.260569	6432.964577	15.266739	-0.056270	4.333334
282.215801	6424.902792	15.271744	-0.056257	4.330714
282.192434	6416.953912	15.276749	-0.056247	4.328129
282.031222	6408.927459	15.281754	-0.056212	4.325517
282.045911	6400.944199	15.286759	-0.056209	4.322918
282.215263	6392.934483	15.291763	-0.056235	4.320310
282.059493	6384.947438	15.296768	-0.056201	4.317706
282.217315	6376.960993	15.301773	-0.056225	4.315103
282.118249	6368.925930	15.306778	-0.056201	4.312480
282.152428	6360.890798	15.311783	-0.056202	4.309856
281.897437	6352.936102	15.316787	-0.056149	4.307255
281.613564	6344.909676	15.321792	-0.056091	4.304629
281.941030	6336.920467	15.326797	-0.056146	4.302018
281.893623	6328.924005	15.331802	-0.056132	4.299400
281.692343	6320.930445	15.336807	-0.056089	4.296781
281.951391	6312.907767	15.341811	-0.056132	4.294154
281.786092	6304.881299	15.346816	-0.056096	4.291520
281.530235	6296.926754	15.351821	-0.056043	4.288908
281.601004	6288.916730	15.356826	-0.056051	4.286279
281.690816	6280.914922	15.361831	-0.056062	4.283651
281.747373	6272.915991	15.366835	-0.056067	4.281022
281.553967	6264.940680	15.371840	-0.056026	4.278397
281.622551	6256.888694	15.376845	-0.056033	4.275747
281.478900	6248.889829	15.381850	-0.056001	4.273111
281.405500	6240.857194	15.386855	-0.055982	4.270464
281.511737	6232.915712	15.391859	-0.055997	4.267846
281.332623	6224.839075	15.396864	-0.055958	4.265179
281.341606	6216.876926	15.401869	-0.055954	4.262551
281.393362	6208.872252	15.406874	-0.055959	4.259907
281.204374	6200.892276	15.411879	-0.055918	4.257267
281.128298	6192.905760	15.416883	-0.055899	4.254624
281.139556	6184.862439	15.421888	-0.055895	4.251962
281.264011	6176.903011	15.426893	-0.055913	4.249327
281.158008	6168.888977	15.431898	-0.055888	4.246670
280.970790	6160.874758	15.436903	-0.055848	4.244011
281.136286	6152.918700	15.441907	-0.055873	4.241373
281.072653	6144.910132	15.446912	-0.055856	4.238713
280.787665	6136.947723	15.451917	-0.055798	4.236065
280.982839	6128.910852	15.456922	-0.055829	4.233395
281.148467	6120.827298	15.461927	-0.055854	4.230708
280.870627	6112.933368	15.466931	-0.055797	4.228077
280.634336	6104.838036	15.471936	-0.055747	4.225379
280.935655	6096.939013	15.476941	-0.055798	4.222749
280.783432	6088.888925	15.481946	-0.055765	4.220063
280.615265	6080.970770	15.486951	-0.055728	4.217419
280.623115	6072.950464	15.491955	-0.055724	4.214741
280.562022	6064.897190	15.496960	-0.055707	4.212049
280.548093	6056.924199	15.501965	-0.055699	4.209383
280.487266	6048.929729	15.506970	-0.055683	4.206708
280.518346	6040.889053	15.511975	-0.055683	4.204017
280.374220	6032.943765	15.516979	-0.055651	4.201354
280.357815	6024.944642	15.521984	-0.055642	4.198672
280.529497	6016.942848	15.526989	-0.055669	4.195990
280.460733	6008.843084	15.531994	-0.055651	4.193271
280.464408	6000.802984	15.536999	-0.055646	4.190571
280.265119	5992.854461	15.542003	-0.055604	4.187897
280.104162	5984.852322	15.547008	-0.055568	4.185204
280.063555	5976.934039	15.552013	-0.055555	4.182540
279.919312	5968.879622	15.557018	-0.055523	4.179826
280.076347	5960.908586	15.562023	-0.055547	4.177142
280.225504	5952.875303	15.567027	-0.055569	4.174435
279.940254	5944.890317	15.572032	-0.055511	4.171738
280.014236	5936.860686	15.577037	-0.055519	4.169028
279.938578	5928.896727	15.582042	-0.055500	4.166337
279.815140	5920.871248	15.587047	-0.055472	4.163623
279.947495	5912.900476	15.592051	-0.055491	4.160928
279.963625	5904.887165	15.597056	-0.055488	4.158216
279.730961	5896.893185	15.602061	-0.055440	4.155506
279.606549	5888.891564	15.607066	-0.055411	4.152792
279.766754	5880.800650	15.612071	-0.055436	4.150050
279.862840	5872.907643	15.617075	-0.055448	4.147373
279.599166	5864.851318	15.622080	-0.055394	4.144634
279.832632	5856.892122	15.627085	-0.055432	4.141932
279.619617	5848.890600	15.632090	-0.055387	4.139209
279.667835	5840.871326	15.637095	-0.055390	4.136481
279.639962	5832.870153	15.642099	-0.055380	4.133756
279.745285	5824.845637	15.647104	-0.055394	4.131024
279.449389	5816.878528	15.652109	-0.055334	4.128304
279.164840	5808.925532	15.657114	-0.055275	4.125587
279.248013	5800.889410	15.662119	-0.055285	4.122845
279.535422	5792.877552	15.667123	-0.055334	4.120111
279.275195	5784.914078	15.672128	-0.055280	4.117386
279.278495	5776.884105	15.677133	-0.055275	4.114639
279.426114	5768.818521	15.682138	-0.055297	4.111880
279.080875	5760.839771	15.687143	-0.055228	4.109143
279.093207	5752.863848	15.692147	-0.055224	4.106409
279.073478	5744.848965	15.697152	-0.055215	4.103660
279.212681	5736.882482	15.702157	-0.055236	4.100928
279.051160	5728.921937	15.707162	-0.055201	4.098191
278.939447	5720.892205	15.712167	-0.055174	4.095430
278.994875	5712.894110	15.717171	-0.055179	4.092680
278.872657	5704.849373	15.722176	-0.055151	4.089910
278.855411	5696.888491	15.727181	-0.055143	4.087169
278.901895	5688.870676	15.732186	-0.055146	4.084406
278.727688	5680.934004	15.737191	-0.055108	4.081667
278.721427	5672.940872	15.742195	-0.055102	4.078909
278.660118	5664.911979	15.747200	-0.055085	4.076135
278.760452	5656.905559	15.752205	-0.055098	4.073370
278.685022	5648.876452	15.757210	-0.055079	4.070593
278.550147	5640.855279	15.762215	-0.055048	4.067816
278.766124	5632.900132	15.767219	-0.055083	4.065064
278.452503	5624.952204	15.772224	-0.055019	4.062306
278.348119	5616.924674	15.777229	-0.054995	4.059521
278.631582	5608.955002	15.782234	-0.055042	4.056760
278.230548	5600.913960	15.787239	-0.054962	4.053962
278.309243	5592.922364	15.792243	-0.054971	4.051187
278.241329	5584.909164	15.797248	-0.054953	4.048400
278.299664	5576.896191	15.802253	-0.054959	4.045613
278.252414	5568.937123	15.807258	-0.054945	4.042841
278.211380	5560.886530	15.812263	-0.054932	4.040036
278.304845	5552.963810	15.817267	-0.054944	4.037275
278.136874	5544.892218	15.822272	-0.054907	4.034456
278.113775	5536.792381	15.827277	-0.054897	4.031628
278.165610	5528.854896	15.832282	-0.054901	4.028856
277.913355	5520.859333	15.837287	-0.054849	4.026057
278.007307	5512.902470	15.842291	-0.054861	4.023274
277.987409	5504.875853	15.847296	-0.054852	4.020464
278.202709	5496.934457	15.852301	-0.054887	4.017685
277.876896	5488.899610	15.857306	-0.054821	4.014863
277.862309	5480.860259	15.862311	-0.054813	4.012042
278.061474	5472.888134	15.867315	-0.054845	4.009247
277.682222	5464.919042	15.872320	-0.054769	4.006441
277.635483	5456.881227	15.877325	-0.054755	4.003614
277.661896	5448.901687	15.882330	-0.054754	4.000807
277.671086	5440.902821	15.887335	-0.054750	3.997991
277.678395	5432.902593	15.892339	-0.054746	3.995173
277.677111	5424.872118	15.897344	-0.054741	3.992341
277.823440	5416.860892	15.902349	-0.054763	3.989517
277.544361	5408.909437	15.907354	-0.054705	3.986705
277.642900	5400.884344	15.912359	-0.054718	3.983871
277.858796	5392.930068	15.917363	-0.054753	3.981062
277.599476	5384.917140	15.922368	-0.054700	3.978223
277.565706	5376.939104	15.927373	-0.054688	3.975397
277.546720	5368.914098	15.932378	-0.054679	3.972554
277.432267	5360.858894	15.937383	-0.054652	3.969695
277.337985	5352.931719	15.942387	-0.054629	3.966881
277.276524	5344.908454	15.947392	-0.054613	3.964031
277.414140	5336.946428	15.952397	-0.054633	3.961204
277.438678	5328.963890	15.957402	-0.054632	3.958366
277.263179	5320.954658	15.962407	-0.054594	3.955512
277.271194	5312.924844	15.967411	-0.054590	3.952653
277.192327	5304.882314	15.972416	-0.054570	3.949785
277.047064	5296.917173	15.977421	-0.054538	3.946942
276.975432	5288.933233	15.982426	-0.054519	3.944092
277.023515	5280.937835	15.987431	-0.054523	3.941237
276.983196	5273.011974	15.992435	-0.054510	3.938403
276.836419	5264.970617	15.997440	-0.054477	3.935524
276.835487	5256.959318	16.002445	-0.054471	3.932657
276.987791	5248.940090	16.007450	-0.054494	3.929787
276.717874	5240.975771	16.012455	-0.054439	3.926927
276.644407	5232.999621	16.017459	-0.054420	3.924065
276.791909	5224.967701	16.022464	-0.054442	3.921184
276.377407	5217.002379	16.027469	-0.054359	3.918315
276.565217	5208.958477	16.032474	-0.054389	3.915427
276.628263	5200.932042	16.037479	-0.054395	3.912540
276.608860	5192.966031	16.042483	-0.054386	3.909671
276.513960	5184.968207	16.047488	-0.054363	3.906788
276.632231	5176.964412	16.052493	-0.054380	3.903904
276.514302	5168.989164	16.057498	-0.054353	3.901024
276.456430	5160.981292	16.062503	-0.054337	3.898131
276.560481	5152.968312	16.067507	-0.054351	3.895238
276.391644	5144.949727	16.072512	-0.054314	3.892334
276.197298	5136.958385	16.077517	-0.054272	3.889438
276.219430	5128.996932	16.082522	-0.054271	3.886555
276.035032	5120.992968	16.087527	-0.054231	3.883651
276.190910	5112.993248	16.092531	-0.054255	3.880752
275.996812	5104.998434	16.097536	-0.054213	3.877846
276.000945	5096.999897	16.102541	-0.054209	3.874940
275.802036	5088.777975	16.107546	-0.054166	3.871947
275.748090	5080.808539	16.112551	-0.054151	3.869046
275.806070	5072.881878	16.117555	-0.054156	3.866161
275.740450	5064.901914	16.122560	-0.054139	3.863252
275.773201	5056.938012	16.127565	-0.054140	3.860349
275.701712	5048.980694	16.132570	-0.054121	3.857444
275.781312	5040.969802	16.137575	-0.054130	3.854519
275.900629	5032.981550	16.142579	-0.054147	3.851602
275.844227	5024.950193	16.147584	-0.054131	3.848664
275.737409	5016.959357	16.152589	-0.054106	3.845736
275.661815	5009.006989	16.157594	-0.054087	3.842822
275.472530	5000.992163	16.162599	-0.054046	3.839879
275.630584	4993.051619	16.167603	-0.054070	3.836969
275.435327	4985.029059	16.172608	-0.054028	3.834020
275.505503	4977.008752	16.177613	-0.054036	3.831074
275.295149	4968.995278	16.182618	-0.053992	3.828123
275.243678	4961.022258	16.187623	-0.053977	3.825188
275.410487	4953.042882	16.192627	-0.054002	3.822252
275.200684	4945.037030	16.197632	-0.053958	3.819297
275.360074	4937.044098	16.202637	-0.053982	3.816352
275.297785	4929.048123	16.207642	-0.053965	3.813399
275.031148	4921.037296	16.212647	-0.053910	3.810434
275.203683	4913.068859	16.217651	-0.053937	3.807491
275.111429	4905.048615	16.222656	-0.053914	3.804522
275.104566	4897.085293	16.227661	-0.053908	3.801572
275.129643	4889.083334	16.232666	-0.053907	3.798607
275.049823	4881.058471	16.237671	-0.053887	3.795629
275.028484	4873.061707	16.242675	-0.053878	3.792661
274.886370	4865.012869	16.247680	-0.053846	3.789668
274.989085	4857.044844	16.252685	-0.053859	3.786708
275.013858	4849.062510	16.257690	-0.053859	3.783738
274.713705	4841.069054	16.262695	-0.053797	3.780755
274.781742	4833.090869	16.267699	-0.053805	3.777784
274.778901	4825.063806	16.272704	-0.053799	3.774790
274.689841	4817.059211	16.277709	-0.053777	3.771800
274.709446	4809.071114	16.282714	-0.053775	3.768817
274.553283	4801.061655	16.287719	-0.053741	3.765819
274.588977	4793.087788	16.292723	-0.053742	3.762837
274.646445	4785.068056	16.297728	-0.053747	3.759835
274.638403	4777.097050	16.302733	-0.053741	3.756848
274.625865	4769.101051	16.307738	-0.053733	3.753849
274.472518	4761.072780	16.312743	-0.053699	3.750832
274.399389	4753.075137	16.317747	-0.053680	3.747827
274.492515	4745.047023	16.322752	-0.053692	3.744811
274.667919	4737.127201	16.327757	-0.053719	3.741835
274.400366	4729.093857	16.332762	-0.053664	3.738804
274.278883	4721.115932	16.337767	-0.053636	3.735795
274.415873	4713.123224	16.342771	-0.053656	3.732783
274.213638	4705.058338	16.347776	-0.053613	3.729735
274.240142	4697.112844	16.352781	-0.053613	3.726734
274.257918	4689.115693	16.357786	-0.053611	3.723711
274.105619	4681.132598	16.362791	-0.053577	3.720686
274.050152	4673.200959	16.367795	-0.053561	3.717681
274.048281	4665.158685	16.372800	-0.053556	3.714633
273.846675	4657.056087	16.377805	-0.053513	3.711555
273.707298	4649.093568	16.382810	-0.053481	3.708529
273.560798	4641.100294	16.387815	-0.053449	3.705488
273.728685	4633.157224	16.392819	-0.053475	3.702472
273.657259	4625.129561	16.397824	-0.053456	3.699416
273.696708	4617.190630	16.402829	-0.053458	3.696393
273.923316	4609.177132	16.407834	-0.053495	3.693344
273.595245	4601.136307	16.412839	-0.053428	3.690268
273.441687	4593.228132	16.417843	-0.053394	3.687245
273.321094	4585.213270	16.422848	-0.053367	3.684179
273.304470	4577.224349	16.427853	-0.053358	3.681123
273.258038	4569.218785	16.432858	-0.053344	3.678058
273.248732	4561.182416	16.437863	-0.053337	3.674979
273.368697	4553.203553	16.442867	-0.053354	3.671923
273.267382	4545.197351	16.447872	-0.053330	3.668848
273.173906	4537.219323	16.452877	-0.053307	3.665781
273.283311	4529.233504	16.457882	-0.053322	3.662715
273.111541	4521.199558	16.462887	-0.053285	3.659619
272.995184	4513.261936	16.467891	-0.053258	3.656560
273.056080	4505.198275	16.472896	-0.053264	3.653454
273.017037	4497.207344	16.477901	-0.053251	3.650371
273.076725	4489.226934	16.482906	-0.053257	3.647292
272.890677	4481.207927	16.487911	-0.053217	3.644189
272.996051	4473.266155	16.492915	-0.053231	3.641121
272.847496	4465.246167	16.497920	-0.053198	3.638014
272.734413	4457.263680	16.502925	-0.053171	3.634919
272.882965	4449.231230	16.507930	-0.053194	3.631809
272.961311	4441.189579	16.512935	-0.053203	3.628691
272.617615	4433.218852	16.517939	-0.053134	3.625587
272.623900	4425.249061	16.522944	-0.053129	3.622489
272.880460	4417.218769	16.527949	-0.053172	3.619373
272.678522	4409.293311	16.532954	-0.053129	3.616282
272.601770	4401.275385	16.537959	-0.053109	3.613155
272.617401	4393.285101	16.542963	-0.053107	3.610039
272.488475	4385.307985	16.547968	-0.053077	3.606922
272.581008	4377.292501	16.552973	-0.053089	3.603793
272.465301	4369.356277	16.557978	-0.053062	3.600687
272.338542	4361.366350	16.562983	-0.053033	3.597556
272.456418	4353.370658	16.567987	-0.053050	3.594428
272.408774	4345.307030	16.572992	-0.053036	3.591265
272.499531	4337.289853	16.577997	-0.053047	3.588122
272.479242	4329.322665	16.583002	-0.053038	3.584993
272.167466	4321.371694	16.588007	-0.052975	3.581858
272.147018	4313.374902	16.593011	-0.052966	3.578712
272.132085	4305.374453	16.598016	-0.052957	3.575561
271.887325	4297.378086	16.603021	-0.052907	3.572402
272.024206	4289.379112	16.608026	-0.052927	3.569251
272.045433	4281.354550	16.613031	-0.052925	3.566084
272.025829	4273.400932	16.618035	-0.052916	3.562940
271.934320	4265.377607	16.623040	-0.052894	3.559764
272.073078	4257.433502	16.628045	-0.052914	3.556623
272.016846	4249.361202	16.633050	-0.052898	3.553423
271.866764	4241.313426	16.638055	-0.052865	3.550227
271.874760	4233.371230	16.643059	-0.052861	3.547075
271.705342	4225.391256	16.648064	-0.052824	3.543900
271.614172	4217.405580	16.653069	-0.052802	3.540721
271.598385	4209.454377	16.658074	-0.052794	3.537556
271.618947	4201.387705	16.663079	-0.052792	3.534343
271.710367	4193.398138	16.668083	-0.052804	3.531160
271.465287	4185.418588	16.673088	-0.052753	3.527969
271.510866	4177.404742	16.678093	-0.052756	3.524769
271.645315	4169.471775	16.683098	-0.052776	3.521601
271.524344	4161.460139	16.688103	-0.052748	3.518392
271.502827	4153.514477	16.693107	-0.052738	3.515208
271.447506	4145.421390	16.698112	-0.052723	3.511962
271.364080	4137.446077	16.703117	-0.052702	3.508759
271.425861	4129.459110	16.708122	-0.052708	3.505553
271.289795	4121.486201	16.713127	-0.052677	3.502344
271.194120	4113.500473	16.718131	-0.052654	3.499127
271.065044	4105.536357	16.723136	-0.052625	3.495916
271.172151	4097.518630	16.728141	-0.052639	3.492687
271.358709	4089.488142	16.733146	-0.052669	3.489453
271.039945	4081.520075	16.738151	-0.052604	3.486225
271.110539	4073.589935	16.743155	-0.052612	3.483021
271.018481	4065.551077	16.748160	-0.052589	3.479765
270.869389	4057.609819	16.753165	-0.052556	3.476544
270.982967	4049.584386	16.758170	-0.052572	3.473295
270.857191	4041.508500	16.763175	-0.052543	3.470014
270.906250	4033.570859	16.768179	-0.052547	3.466792
270.793582	4025.559824	16.773184	-0.052521	3.463531
270.813694	4017.554213	16.778189	-0.052519	3.460274
270.870525	4009.619087	16.783194	-0.052524	3.457044
270.543180	4001.587484	16.788199	-0.052458	3.453759
270.541810	3993.581795	16.793203	-0.052452	3.450493
270.440141	3985.609359	16.798208	-0.052428	3.447233
270.415239	3977.597853	16.803213	-0.052418	3.443957
270.301831	3969.633190	16.808218	-0.052391	3.440694
270.410936	3961.643583	16.813223	-0.052406	3.437425
270.446893	3953.639330	16.818227	-0.052408	3.434144
270.453207	3945.608637	16.823232	-0.052404	3.430848
270.333272	3937.637775	16.828237	-0.052376	3.427570
270.319210	3929.635559	16.833242	-0.052368	3.424279
270.134365	3921.661915	16.838247	-0.052328	3.420991
270.278292	3913.700741	16.843251	-0.052350	3.417716
270.248905	3905.660813	16.848256	-0.052339	3.414399
270.096936	3897.680445	16.853261	-0.052305	3.411100
269.968250	3889.717271	16.858266	-0.052276	3.407805
270.059645	3881.697527	16.863271	-0.052287	3.404492
270.090876	3873.748611	16.868275	-0.052288	3.401202
269.944769	3865.770239	16.873280	-0.052255	3.397891
269.846624	3857.741534	16.878285	-0.052232	3.394557
269.864065	3849.668223	16.883290	-0.052230	3.391206
269.691648	3841.691698	16.888295	-0.052192	3.387885
269.819290	3833.712769	16.893299	-0.052210	3.384570
269.935950	3825.772504	16.898304	-0.052227	3.381267
269.731249	3817.783338	16.903309	-0.052183	3.377930
269.720633	3809.784187	16.908314	-0.052176	3.374592
269.609283	3801.778376	16.913319	-0.052150	3.371244
269.800534	3793.807001	16.918323	-0.052180	3.367918
269.610705	3785.797713	16.923328	-0.052139	3.364559
269.386252	3777.860566	16.928333	-0.052092	3.361226
269.516767	3769.868909	16.933338	-0.052111	3.357880
269.508617	3761.846550	16.938343	-0.052104	3.354512
269.217270	3753.852239	16.943347	-0.052045	3.351143
269.328661	3745.830537	16.948352	-0.052060	3.347773
269.340957	3737.842501	16.953357	-0.052057	3.344410
269.407425	3729.878523	16.958362	-0.052064	3.341056
269.188712	3721.895568	16.963367	-0.052018	3.337680
269.349483	3713.889902	16.968371	-0.052043	3.334305
269.147711	3705.872303	16.973376	-0.052000	3.330909
268.949201	3697.895882	16.978381	-0.051957	3.327526
269.160514	3689.903457	16.983386	-0.051991	3.324148
268.909169	3681.932562	16.988391	-0.051939	3.320759
268.738004	3674.002552	16.993395	-0.051902	3.317387
268.767401	3665.956471	16.998400	-0.051902	3.313969
268.839699	3657.898739	17.003405	-0.051910	3.310544
268.704234	3649.971101	17.008410	-0.051880	3.307164
268.542209	3641.952236	17.013415	-0.051844	3.303740
268.510575	3634.007661	17.018419	-0.051833	3.300349
268.456614	3626.012625	17.023424	-0.051817	3.296933
268.439875	3618.011626	17.028429	-0.051809	3.293511
268.603361	3610.001315	17.033434	-0.051834	3.290089
268.532964	3602.008653	17.038439	-0.051816	3.286662
268.402379	3594.079266	17.043443	-0.051786	3.283256
268.502537	3586.040660	17.048448	-0.051799	3.279809
268.392160	3578.108664	17.053453	-0.051773	3.276396
268.491524	3570.072398	17.058458	-0.051786	3.272942
268.126969	3562.058499	17.063463	-0.051713	3.269476
268.405079	3554.083735	17.068467	-0.051760	3.266049
268.396565	3546.075426	17.073472	-0.051753	3.262592
268.235751	3538.092439	17.078477	-0.051717	3.259137
268.170729	3530.143845	17.083482	-0.051700	3.255697
268.124513	3522.121244	17.088487	-0.051686	3.252221
267.902246	3514.150814	17.093491	-0.051639	3.248758
267.913727	3506.148727	17.098496	-0.051636	3.245286
268.064941	3498.163831	17.103501	-0.051659	3.241824
267.983465	3490.178102	17.108506	-0.051638	3.238348
267.816762	3482.201020	17.113511	-0.051602	3.234869
268.001703	3474.131141	17.118515	-0.051631	3.231360
268.107675	3466.138104	17.123520	-0.051645	3.227877
267.815541	3458.166553	17.128525	-0.051585	3.224384
267.887207	3450.236813	17.133530	-0.051594	3.220920
267.698507	3442.249456	17.138535	-0.051553	3.217416
267.739539	3434.240037	17.143539	-0.051555	3.213909
267.599724	3426.222949	17.148544	-0.051524	3.210387
267.736412	3418.249030	17.153549	-0.051544	3.206891
267.650146	3410.277150	17.158554	-0.051523	3.203383
267.494532	3402.312823	17.163559	-0.051488	3.199872
267.468802	3394.350647	17.168563	-0.051478	3.196363
267.562421	3386.316535	17.173568	-0.051490	3.192823
267.476342	3378.306309	17.178573	-0.051469	3.189283
267.556297	3370.328688	17.183578	-0.051478	3.185760
267.233849	3362.373004	17.188583	-0.051413	3.182226
267.297277	3354.394226	17.193587	-0.051419	3.178694
267.287450	3346.364492	17.198592	-0.051412	3.175133
267.099928	3338.384789	17.203597	-0.051372	3.171582
267.248358	3330.402047	17.208602	-0.051394	3.168040
266.978783	3322.407590	17.213607	-0.051339	3.164471
267.221659	3314.424453	17.218611	-0.051378	3.160925
267.174443	3306.448246	17.223616	-0.051364	3.157365
267.110259	3298.447070	17.228621	-0.051347	3.153790
267.074768	3290.444528	17.233626	-0.051335	3.150211
266.993385	3282.447216	17.238631	-0.051315	3.146629
267.077170	3274.483283	17.243635	-0.051325	3.143064
266.894388	3266.489098	17.248640	-0.051285	3.139471
266.836166	3258.528748	17.253645	-0.051269	3.135893
266.878401	3250.527367	17.258650	-0.051272	3.132298
266.839919	3242.518161	17.263655	-0.051259	3.128692
266.715067	3234.559988	17.268659	-0.051231	3.125100
266.751597	3226.586745	17.273664	-0.051232	3.121505
266.736439	3218.605695	17.278669	-0.051224	3.117899
266.805360	3210.614487	17.283674	-0.051231	3.114289
266.779234	3202.563408	17.288679	-0.051221	3.110643
266.768371	3194.620085	17.293683	-0.051214	3.107043
266.683582	3186.645236	17.298688	-0.051193	3.103420
266.509384	3178.646120	17.303693	-0.051155	3.099778
266.679164	3170.693994	17.308698	-0.051181	3.096169
266.279643	3162.677444	17.313703	-0.051101	3.092501
266.343177	3154.698546	17.318707	-0.051108	3.088866
266.381938	3146.701433	17.323712	-0.051110	3.085218
266.061708	3138.755543	17.328717	-0.051045	3.081572
266.149572	3130.779221	17.333722	-0.051056	3.077927
266.100243	3122.762890	17.338727	-0.051041	3.074252
266.017771	3114.702394	17.343731	-0.051020	3.070552
265.976137	3106.718167	17.348736	-0.051007	3.066884
265.800527	3098.748377	17.353741	-0.050969	3.063212
266.011414	3090.773090	17.358746	-0.051003	3.059551
265.978600	3082.813948	17.363751	-0.050992	3.055881
265.775420	3074.839277	17.368755	-0.050948	3.052192
265.726067	3066.845016	17.373760	-0.050934	3.048497
265.920499	3058.817801	17.378765	-0.050965	3.044794
265.871656	3050.887374	17.383770	-0.050950	3.041119
265.663688	3042.925822	17.388775	-0.050906	3.037418
265.689314	3034.931716	17.393779	-0.050906	3.033709
265.646056	3026.917609	17.398784	-0.050892	3.029982
265.596677	3018.930786	17.403789	-0.050878	3.026263
265.664727	3010.956298	17.408794	-0.050885	3.022551
265.279280	3002.990784	17.413799	-0.050808	3.018816
265.292353	2995.027695	17.418803	-0.050805	3.015098
265.287031	2987.005630	17.423808	-0.050799	3.011346
265.347806	2978.999287	17.428813	-0.050805	3.007600
265.333254	2971.039433	17.433818	-0.050797	3.003868
265.208081	2963.060595	17.438823	-0.050768	3.000117
265.242117	2955.118806	17.443827	-0.050769	2.996386
265.290985	2947.078573	17.448832	-0.050773	2.992605
264.875435	2939.105651	17.453837	-0.050690	2.988827
265.064722	2931.103931	17.458842	-0.050720	2.985062
264.847227	2923.125101	17.463847	-0.050674	2.981282
264.967901	2915.160706	17.468851	-0.050691	2.977521
265.159933	2907.153232	17.473856	-0.050721	2.973739
264.854346	2899.185385	17.478861	-0.050659	2.969946
264.745453	2891.225861	17.483866	-0.050634	2.966161
264.766688	2883.236332	17.488871	-0.050632	2.962364
264.784770	2875.256721	17.493875	-0.050630	2.958567
264.576718	2867.296652	17.498880	-0.050586	2.954762
264.537902	2859.278339	17.503885	-0.050573	2.950934
264.860408	2851.269260	17.508890	-0.050628	2.947123
264.759598	2843.290788	17.513895	-0.050604	2.943301
264.540165	2835.341468	17.518899	-0.050558	2.939481
264.678891	2827.361716	17.523904	-0.050578	2.935660
264.407857	2819.379739	17.528909	-0.050523	2.931812
264.486999	2811.379919	17.533914	-0.050532	2.927969
264.495331	2803.386639	17.538919	-0.050528	2.924120
264.478997	2795.442165	17.543923	-0.050520	2.920288
264.264052	2787.490494	17.548928	-0.050474	2.916437
264.116132	2779.423994	17.553933	-0.050441	2.912528
264.359270	2771.403339	17.558938	-0.050481	2.908658
264.284150	2763.420593	17.563943	-0.050462	2.904784
264.268649	2755.507508	17.568947	-0.050454	2.900942
264.097276	2747.547065	17.573952	-0.050416	2.897063
264.144588	2739.539810	17.578957	-0.050420	2.893168
263.870174	2731.580310	17.583962	-0.050364	2.889274
263.766585	2723.580091	17.588967	-0.050339	2.885363
263.952139	2715.604527	17.593971	-0.050368	2.881475
263.866163	2707.639328	17.598976	-0.050347	2.877573
263.737479	2699.668110	17.603981	-0.050317	2.873659
263.914352	2691.635460	17.608986	-0.050345	2.869727
263.842428	2683.660044	17.613991	-0.050326	2.865804
263.848733	2675.699478	17.618995	-0.050322	2.861887
263.771256	2667.731379	17.624000	-0.050302	2.857956
263.840106	2659.738186	17.629005	-0.050310	2.854016
263.837181	2651.727479	17.634010	-0.050304	2.850058
263.579403	2643.812853	17.639015	-0.050250	2.846127
263.712026	2635.832945	17.644019	-0.050270	2.842181
263.378820	2627.889263	17.649024	-0.050202	2.838220
263.286751	2619.891128	17.654029	-0.050180	2.834241
263.310018	2611.867313	17.659034	-0.050179	2.830250
263.427202	2603.852228	17.664039	-0.050195	2.826263
263.219507	2595.917406	17.669043	-0.050151	2.822292
263.153473	2587.965786	17.674048	-0.050134	2.818315
263.174346	2579.974934	17.679053	-0.050132	2.814317
263.262035	2571.958487	17.684058	-0.050143	2.810305
263.177776	2563.989389	17.689063	-0.050122	2.806301
263.268572	2556.013397	17.694067	-0.050134	2.802298
263.106945	2548.053096	17.699072	-0.050098	2.798282
262.836551	2540.105127	17.704077	-0.050043	2.794261
262.924416	2532.083364	17.709082	-0.050054	2.790217
263.053672	2524.092449	17.714087	-0.050072	2.786186
263.053646	2516.129286	17.719091	-0.050067	2.782155
262.865263	2508.193435	17.724096	-0.050027	2.778121
262.639939	2500.220672	17.729101	-0.049979	2.774060
262.646568	2492.219729	17.734106	-0.049975	2.769993
262.429869	2484.252985	17.739111	-0.049929	2.765924
262.575515	2476.279486	17.744115	-0.049951	2.761867
262.790881	2468.281945	17.749120	-0.049986	2.757796
262.445417	2460.307737	17.754125	-0.049916	2.753697
262.344713	2452.276570	17.759130	-0.049892	2.749577
262.278414	2444.303309	17.764135	-0.049874	2.745483
262.360239	2436.353018	17.769139	-0.049884	2.741404
262.316275	2428.383314	17.774144	-0.049871	2.737301
262.226785	2420.404339	17.779149	-0.049849	2.733185
262.515004	2412.415564	17.784154	-0.049897	2.729080
262.311976	2404.449978	17.789159	-0.049854	2.724951
262.211361	2396.520544	17.794163	-0.049830	2.720840
262.142103	2388.547050	17.799168	-0.049812	2.716703
262.051263	2380.542052	17.804173	-0.049789	2.712541
262.332902	2372.539604	17.809178	-0.049836	2.708398
262.204952	2364.568392	17.814183	-0.049807	2.704238
262.044619	2356.634934	17.819187	-0.049772	2.700091
261.861847	2348.697942	17.824192	-0.049733	2.695933
261.720636	2340.683023	17.829197	-0.049701	2.691731
261.846365	2332.703858	17.834202	-0.049719	2.687558
261.423675	2324.780105	17.839207	-0.049635	2.683372
261.575990	2316.795203	17.844211	-0.049658	2.679185
261.645232	2308.832173	17.849216	-0.049666	2.674997
261.659723	2300.778179	17.854221	-0.049663	2.670751
261.610223	2292.825686	17.859226	-0.049648	2.666548
261.530893	2284.848110	17.864231	-0.049628	2.662323
261.367195	2276.910610	17.869235	-0.049592	2.658107
261.388388	2268.917936	17.874240	-0.049591	2.653867
261.466184	2260.906149	17.879245	-0.049600	2.649613
261.557152	2252.948633	17.884250	-0.049612	2.645383
261.284192	2245.015416	17.889255	-0.049556	2.641135
261.356633	2237.059071	17.894259	-0.049564	2.636891
261.315102	2229.060425	17.899264	-0.049551	2.632609
261.248727	2221.079041	17.904269	-0.049533	2.628328
261.057956	2213.136817	17.909274	-0.049492	2.624053
261.055161	2205.148988	17.914279	-0.049486	2.619759
261.048981	2197.214938	17.919283	-0.049480	2.615487
260.971361	2189.220298	17.924288	-0.049460	2.611170
260.676246	2181.277220	17.929293	-0.049400	2.606859
260.896552	2173.282990	17.934298	-0.049435	2.602548
260.747609	2165.321442	17.939303	-0.049402	2.598222
260.754675	2157.323014	17.944307	-0.049398	2.593880
260.856416	2149.168965	17.949312	-0.049412	2.589453
260.662323	2141.255393	17.954317	-0.049370	2.585128
260.617854	2133.347833	17.959322	-0.049357	2.580810
260.489486	2125.413566	17.964327	-0.049327	2.576465
260.506101	2117.426369	17.969331	-0.049325	2.572093
260.298353	2109.491825	17.974336	-0.049281	2.567726
260.335939	2101.508698	17.979341	-0.049283	2.563343
260.303599	2093.578931	17.984346	-0.049271	2.558977
260.200057	2085.625047	17.989351	-0.049247	2.554585
260.104836	2077.629335	17.994355	-0.049224	2.550163
260.159434	2069.643460	17.999360	-0.049229	2.545749
260.012613	2061.697018	18.004365	-0.049196	2.541335
260.016510	2053.750603	18.009370	-0.049191	2.536924
260.053849	2045.755958	18.014375	-0.049193	2.532481
259.953544	2037.812781	18.019379	-0.049169	2.528049
260.020556	2029.835627	18.024384	-0.049176	2.523602
259.909436	2021.891412	18.029389	-0.049150	2.519153
260.111856	2013.917428	18.034394	-0.049182	2.514702
259.907472	2005.912426	18.039399	-0.049139	2.510196
259.827653	1997.962214	18.044403	-0.049119	2.505722
259.916491	1989.999235	18.049408	-0.049130	2.501245
259.717149	1982.050889	18.054413	-0.049087	2.496748
259.572967	1974.098810	18.059418	-0.049055	2.492244
259.557035	1966.106834	18.064423	-0.049047	2.487718
259.654835	1958.150678	18.069427	-0.049060	2.483214
259.509921	1950.228343	18.074432	-0.049028	2.478702
259.320927	1942.257476	18.079437	-0.048987	2.474151
259.461812	1934.259776	18.084442	-0.049008	2.469601
259.291152	1926.275330	18.089447	-0.048971	2.465026
259.112223	1918.363017	18.094451	-0.048932	2.460484
259.187588	1910.402225	18.099456	-0.048941	2.455925
259.063776	1902.423626	18.104461	-0.048912	2.451332
258.997182	1894.475032	18.109466	-0.048895	2.446752
259.057348	1886.492781	18.114471	-0.048900	2.442154
259.251500	1878.530828	18.119475	-0.048931	2.437569
258.938484	1870.589690	18.124480	-0.048868	2.432948
259.010003	1862.537499	18.129485	-0.048876	2.428284
258.911484	1854.608020	18.134490	-0.048852	2.423669
258.687969	1846.672209	18.139495	-0.048805	2.419032
258.879081	1838.695703	18.144499	-0.048835	2.414394
258.861339	1830.726633	18.149504	-0.048827	2.409736
258.682362	1822.783232	18.154509	-0.048788	2.405071
258.547907	1814.873876	18.159514	-0.048758	2.400420
258.407022	1806.923213	18.164519	-0.048726	2.395736
258.396991	1798.929136	18.169523	-0.048719	2.391026
258.333124	1790.957478	18.174528	-0.048702	2.386317
258.253648	1783.006581	18.179533	-0.048681	2.381609
258.274463	1775.069313	18.184538	-0.048680	2.376908
258.383984	1767.073026	18.189543	-0.048695	2.372170
258.356726	1759.113394	18.194547	-0.048685	2.367433
258.313010	1751.177412	18.199552	-0.048671	2.362700
258.228587	1743.247962	18.204557	-0.048650	2.357957
258.150036	1735.294628	18.209562	-0.048630	2.353191
257.841572	1727.332901	18.214567	-0.048567	2.348392
257.881928	1719.351805	18.219571	-0.048570	2.343600
257.873820	1711.414810	18.224576	-0.048563	2.338820
257.651505	1703.472996	18.229581	-0.048516	2.334010
257.630013	1695.497670	18.234586	-0.048507	2.329186
257.619348	1687.527614	18.239591	-0.048499	2.324357
257.490571	1679.613094	18.244595	-0.048470	2.319541
257.622688	1671.657908	18.249600	-0.048489	2.314712
257.745650	1663.630953	18.254605	-0.048507	2.309829
257.754135	1655.698842	18.259610	-0.048503	2.304984
257.684785	1647.744151	18.264615	-0.048485	2.300108
257.671378	1639.824094	18.269619	-0.048477	2.295247
257.507341	1631.871028	18.274624	-0.048441	2.290344
257.250261	1623.929187	18.279629	-0.048388	2.285428
257.378936	1615.991774	18.284634	-0.048407	2.280538
257.186890	1608.054620	18.289639	-0.048365	2.275610
257.232369	1600.024723	18.294643	-0.048369	2.270634
257.092437	1592.078466	18.299648	-0.048337	2.265683
257.058809	1584.142172	18.304653	-0.048326	2.260737
257.220633	1576.187608	18.309658	-0.048350	2.255785
256.918793	1568.256824	18.314663	-0.048289	2.250797
256.899395	1560.304465	18.319667	-0.048280	2.245809
256.798503	1552.379407	18.324672	-0.048256	2.240820
256.672831	1544.438381	18.329677	-0.048227	2.235807
256.687851	1536.465419	18.334682	-0.048224	2.230776
256.694332	1528.492147	18.339687	-0.048220	2.225732
256.676618	1520.574995	18.344691	-0.048212	2.220710
256.451152	1512.665189	18.349696	-0.048164	2.215663
256.676153	1504.654376	18.354701	-0.048201	2.210580
256.615219	1496.727977	18.359706	-0.048184	2.205514
256.385279	1488.808814	18.364711	-0.048136	2.200425
256.666509	1480.848316	18.369715	-0.048183	2.195345
256.651491	1472.872264	18.374720	-0.048175	2.190215
256.313628	1464.949244	18.379725	-0.048107	2.185079
256.331689	1457.027913	18.384730	-0.048105	2.179964
256.460230	1449.054070	18.389735	-0.048123	2.174813
256.372193	1441.123801	18.394739	-0.048102	2.169658
256.148254	1433.204455	18.399744	-0.048055	2.164485
256.158332	1425.266275	18.404749	-0.048051	2.159309
256.223947	1417.328917	18.409754	-0.048058	2.154127
255.744770	1409.406157	18.414759	-0.047964	2.148891
255.777003	1401.455462	18.419763	-0.047964	2.143671
255.863479	1393.508736	18.424768	-0.047975	2.138447
255.682430	1385.580779	18.429773	-0.047936	2.133196
255.760161	1377.624891	18.434778	-0.047945	2.127939
255.687664	1369.686002	18.439783	-0.047926	2.122666
255.575401	1361.791363	18.444787	-0.047900	2.117405
255.424462	1353.823768	18.449792	-0.047867	2.112079
255.378837	1345.834554	18.454797	-0.047853	2.106735
255.375612	1337.917194	18.459802	-0.047847	2.101429
255.248529	1330.005033	18.464807	-0.047818	2.096102
255.210215	1322.052727	18.469811	-0.047806	2.090743
255.244198	1314.111241	18.474816	-0.047807	2.085384
255.092065	1306.200152	18.479821	-0.047773	2.080014
255.016542	1298.294984	18.484826	-0.047754	2.074641
254.966709	1290.333039	18.489831	-0.047739	2.069218
255.175208	1282.366367	18.494835	-0.047772	2.063804
254.985976	1274.478580	18.499840	-0.047732	2.058389
254.992805	1266.540457	18.504845	-0.047728	2.052946
255.051388	1258.598771	18.509850	-0.047733	2.047490
254.692895	1250.724263	18.514855	-0.047661	2.042024
254.636084	1242.802170	18.519859	-0.047645	2.036541
254.959194	1234.800087	18.524864	-0.047700	2.031027
254.823838	1226.856304	18.529869	-0.047670	2.025491
254.716014	1218.973197	18.534874	-0.047644	2.019985
254.691461	1211.048933	18.539879	-0.047634	2.014444
254.765378	1203.097644	18.544883	-0.047643	2.008879
254.448321	1195.225561	18.549888	-0.047579	2.003314
254.392139	1187.303705	18.554893	-0.047563	1.997725
254.598868	1179.348665	18.559898	-0.047596	1.992124
254.179848	1171.453881	18.564903	-0.047513	1.986484
254.247044	1163.521705	18.569907	-0.047520	1.980854
254.203289	1155.611925	18.574912	-0.047506	1.975211
254.130389	1147.668486	18.579917	-0.047487	1.969525
254.122713	1139.757836	18.584922	-0.047481	1.963853
254.091258	1131.851898	18.589927	-0.047470	1.958165
254.059260	1123.906752	18.594931	-0.047458	1.952432
253.851328	1115.979872	18.599936	-0.047414	1.946677
253.814692	1108.049764	18.604941	-0.047402	1.940921
253.947153	1100.138309	18.609946	-0.047421	1.935180
253.819925	1092.200235	18.614951	-0.047392	1.929373
253.827934	1084.291929	18.619955	-0.047389	1.923586
253.756627	1076.409807	18.624960	-0.047370	1.917792
253.677595	1068.481577	18.629965	-0.047350	1.911946
253.716826	1060.567536	18.634970	-0.047352	1.906105
253.580637	1052.674824	18.639975	-0.047321	1.900242
253.501786	1044.777296	18.644979	-0.047301	1.894364
253.446137	1036.852700	18.649984	-0.047286	1.888450
253.377715	1028.947172	18.654989	-0.047268	1.882531
253.417662	1021.060413	18.659994	-0.047270	1.876619
253.139916	1013.154737	18.664999	-0.047213	1.870638
253.107849	1005.236822	18.670003	-0.047202	1.864656
253.269453	997.314892	18.675008	-0.047226	1.858675
253.217938	989.399229	18.680013	-0.047211	1.852654
253.009452	981.526010	18.685018	-0.047167	1.846628
252.991783	973.618373	18.690023	-0.047159	1.840578
252.998901	965.725186	18.695027	-0.047155	1.834522
252.809019	957.835701	18.700032	-0.047114	1.828426
252.709233	949.924078	18.705037	-0.047090	1.822302
252.744786	942.042948	18.710042	-0.047092	1.816198
252.465278	934.161559	18.715047	-0.047034	1.810035
252.440863	926.265377	18.720051	-0.047024	1.803871
252.494939	918.368889	18.725056	-0.047029	1.797694
252.439393	910.429773	18.730061	-0.047013	1.791449
252.218944	902.538803	18.735066	-0.046967	1.785200
252.028603	894.675865	18.740071	-0.046926	1.778955
252.411017	886.720933	18.745075	-0.046992	1.772686
252.241602	878.852529	18.750080	-0.046955	1.766395
251.953032	871.007862	18.755085	-0.046896	1.760086
251.990797	863.123497	18.760090	-0.046898	1.753763
252.102082	855.184220	18.765095	-0.046914	1.747382
251.903112	847.339320	18.770099	-0.046871	1.741014
251.871128	839.472313	18.775104	-0.046860	1.734627
251.825441	831.583035	18.780109	-0.046846	1.728196
251.802595	823.710188	18.785114	-0.046837	1.721757
251.903328	815.814468	18.790119	-0.046850	1.715291
251.855580	807.922949	18.795123	-0.046836	1.708785
251.646623	800.079171	18.800128	-0.046792	1.702273
251.475252	792.223208	18.805133	-0.046755	1.695730
251.311849	784.365938	18.810138	-0.046719	1.689162
251.307804	776.480773	18.815143	-0.046713	1.682566
251.117886	768.646835	18.820147	-0.046672	1.675963
251.027293	760.765687	18.825152	-0.046650	1.669306
251.066902	752.870846	18.830157	-0.046652	1.662629
251.124867	745.008365	18.835162	-0.046658	1.655955
251.007025	737.135710	18.840167	-0.046630	1.649221
251.054386	729.271659	18.845171	-0.046634	1.642490
251.124205	721.420757	18.850176	-0.046642	1.635745
250.853067	713.528190	18.855181	-0.046586	1.628890
250.787757	705.684082	18.860186	-0.046569	1.622076
250.651553	697.832975	18.865191	-0.046538	1.615217
250.502533	689.998297	18.870195	-0.046505	1.608341
250.472721	682.146870	18.875200	-0.046494	1.601438
250.428648	674.298190	18.880205	-0.046481	1.594505
250.444486	666.435843	18.885210	-0.046478	1.587539
250.190122	658.623805	18.890215	-0.046426	1.580548
250.283383	650.759456	18.895219	-0.046438	1.573529
250.206126	642.923220	18.900224	-0.046418	1.566479
250.051231	635.105130	18.905229	-0.046384	1.559403
250.119983	627.252225	18.910234	-0.046392	1.552295
250.144894	619.380146	18.915239	-0.046391	1.545131
249.892439	611.591513	18.920243	-0.046339	1.537968
249.969541	603.740419	18.925248	-0.046348	1.530764
249.699047	595.940986	18.930253	-0.046292	1.523521
249.849224	588.102819	18.935258	-0.046315	1.516271
249.722308	580.277727	18.940263	-0.046286	1.508956
249.838345	572.433035	18.945267	-0.046302	1.501625
249.644667	564.655194	18.950272	-0.046261	1.494272
249.423421	556.842263	18.955277	-0.046215	1.486846
249.522052	549.030558	18.960282	-0.046228	1.479434
249.316185	541.217119	18.965287	-0.046184	1.471935
249.159423	533.393766	18.970291	-0.046150	1.464395
249.149642	525.590508	18.975296	-0.046143	1.456859
248.954266	517.803842	18.980301	-0.046101	1.449271
249.179432	509.962977	18.985306	-0.046138	1.441657
248.962993	502.206278	18.990311	-0.046092	1.434014
248.814332	494.411227	18.995315	-0.046059	1.426303
248.765266	486.641785	19.000320	-0.046045	1.418592
248.590947	478.856865	19.005325	-0.046007	1.410803
248.753432	471.050247	19.010330	-0.046032	1.403004
248.516034	463.308386	19.015335	-0.045983	1.395161
248.462371	455.504963	19.020339	-0.045968	1.387241
248.444137	447.736644	19.025344	-0.045959	1.379318
248.427479	439.951877	19.030349	-0.045951	1.371333
248.485512	432.182397	19.035354	-0.045956	1.363329
248.138890	424.479010	19.040359	-0.045887	1.355276
247.977843	416.719779	19.045363	-0.045851	1.347150
248.161131	408.934924	19.050368	-0.045880	1.339007
248.107289	401.175350	19.055373	-0.045865	1.330800
247.940157	393.462861	19.060378	-0.045829	1.322571
247.902047	385.699279	19.065383	-0.045816	1.314259
247.809348	377.851284	19.070387	-0.045794	1.305794
247.707989	370.156989	19.075392	-0.045770	1.297438
247.545490	362.438353	19.080397	-0.045734	1.288991
247.423619	354.743701	19.085402	-0.045707	1.280521
247.200566	347.057547	19.090407	-0.045660	1.271986
247.294610	339.313740	19.095411	-0.045672	1.263388
247.205318	331.629908	19.100416	-0.045650	1.254764
246.930949	323.949763	19.105421	-0.045594	1.246049
246.918881	316.268196	19.110426	-0.045587	1.237321
246.802888	308.563500	19.115431	-0.045560	1.228485
246.710591	300.884886	19.120435	-0.045538	1.219619
246.562770	293.224113	19.125440	-0.045505	1.210699
246.741847	285.504692	19.130445	-0.045533	1.201708
246.763338	277.838610	19.135450	-0.045532	1.192681
246.675321	270.179678	19.140455	-0.045510	1.183571
246.394303	262.580139	19.145459	-0.045453	1.174423
246.221616	254.950422	19.150464	-0.045416	1.165188
246.146568	247.321042	19.155469	-0.045397	1.155900
246.091098	239.652432	19.160474	-0.045381	1.146493
246.007717	232.031182	19.165479	-0.045361	1.137061
245.855001	224.421678	19.170483	-0.045327	1.127550
245.705841	216.843969	19.175488	-0.045294	1.117998
245.638238	209.228412	19.180493	-0.045276	1.108334
245.706081	201.627763	19.185498	-0.045284	1.098634
245.545535	194.062009	19.190503	-0.045249	1.088842
245.411953	186.509740	19.195507	-0.045219	1.078984
245.368905	178.937016	19.200512	-0.045206	1.069029
245.280763	171.381134	19.205517	-0.045184	1.058993
245.141664	163.855903	19.210522	-0.045153	1.048889
245.328768	156.283184	19.215527	-0.045183	1.038700
245.295969	148.761487	19.220531	-0.045172	1.028428
244.921685	141.318816	19.225536	-0.045097	1.018079
244.635813	133.848641	19.230541	-0.045039	1.007607
244.545414	126.383867	19.235546	-0.045017	0.997080
244.352278	118.885402	19.240551	-0.044976	0.986367
244.160534	111.445897	19.245555	-0.044936	0.975622
244.362476	103.952773	19.250560	-0.044968	0.964779
244.103166	96.558225	19.255565	-0.044915	0.953840
244.051349	89.140544	19.260570	-0.044900	0.942793
243.798711	81.771148	19.265575	-0.044848	0.931636
243.781763	74.383772	19.270579	-0.044840	0.920378
243.674022	67.023160	19.275584	-0.044815	0.908998
243.366145	59.934304	19.280589	-0.044753	0.897845