Fri Mar 12 11:30:33 2021


Number of Points = 3626

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.624294	0.004903	0.000000	-0.000000	0.718646
0.612268	0.004183	0.005005	0.000002	0.718640
0.683727	-0.004289	0.010010	-0.000011	0.718648
0.403111	0.041998	0.015014	0.000041	0.718641
0.424088	0.041567	0.020019	0.000038	0.718647
0.660420	-0.002754	0.025024	-0.000006	0.718642
0.443941	0.036222	0.030029	0.000034	0.718643
0.629423	0.008548	0.035034	-0.000000	0.718653
0.360670	0.050627	0.040038	0.000050	0.718641
0.465236	0.036811	0.045043	0.000031	0.718651
0.605094	0.009316	0.050048	0.000005	0.718645
0.532189	0.021574	0.055053	0.000018	0.718643
0.597289	0.012099	0.060058	0.000006	0.718647
0.470655	0.030171	0.065062	0.000030	0.718638
0.522290	0.026810	0.070067	0.000021	0.718649
0.557760	0.018066	0.075072	0.000014	0.718644
0.479181	-0.048636	0.080077	0.000029	0.718485
0.412628	-0.103235	0.085082	0.000042	0.718353
0.466544	-0.115263	0.090086	0.000032	0.718348
0.428845	-0.105324	0.095091	0.000039	0.718354
0.314825	-0.086335	0.100096	0.000060	0.718351
0.483950	-0.116750	0.105101	0.000029	0.718351
0.529739	-0.121917	0.110106	0.000021	0.718356
0.580428	-0.272371	0.115110	0.000011	0.718077
0.515421	-0.289565	0.120115	0.000024	0.718019
0.411358	-0.271835	0.125120	0.000043	0.718018
0.565666	-0.301823	0.130125	0.000015	0.718012
0.666539	-0.315145	0.135130	-0.000004	0.718021
0.584856	-0.448076	0.140134	0.000011	0.717729
0.682101	-0.478126	0.145139	-0.000006	0.717704
0.425692	-0.431799	0.150144	0.000041	0.717705
0.256612	-0.404067	0.155149	0.000073	0.717700
0.561914	-0.563984	0.160154	0.000016	0.717491
0.327463	-0.579388	0.165158	0.000060	0.717378
0.499711	-0.606809	0.170163	0.000028	0.717384
0.412347	-0.593315	0.175168	0.000045	0.717380
0.373902	-0.726477	0.180173	0.000052	0.717102
0.413101	-0.739786	0.185178	0.000045	0.717090
0.417556	-0.744973	0.190182	0.000044	0.717081
0.532482	-0.850974	0.195187	0.000023	0.716911
0.455742	-0.915953	0.200192	0.000038	0.716755
0.335297	-0.896169	0.205197	0.000060	0.716751
0.563860	-0.999903	0.210202	0.000018	0.716626
0.437652	-1.068966	0.215206	0.000042	0.716445
0.398727	-1.058460	0.220211	0.000049	0.716452
0.312537	-1.130571	0.225216	0.000065	0.716278
0.479533	-1.234800	0.230221	0.000034	0.716130
0.584639	-1.249520	0.235226	0.000015	0.716138
0.254005	-1.304633	0.240230	0.000077	0.715912
0.245659	-1.316393	0.245235	0.000078	0.715885
0.247481	-1.351427	0.250240	0.000078	0.715816
0.222093	-1.482987	0.255245	0.000083	0.715546
0.376059	-1.506887	0.260250	0.000055	0.715553
0.248405	-1.602825	0.265254	0.000079	0.715317
0.163874	-1.628349	0.270259	0.000095	0.715236
0.285501	-1.704838	0.275264	0.000072	0.715127
0.139744	-1.790203	0.280269	0.000099	0.714906
-0.025224	-1.756542	0.285274	0.000130	0.714914
-0.127535	-1.894235	0.290278	0.000150	0.714605
-0.236668	-1.871898	0.295283	0.000170	0.714610
-0.217003	-1.988027	0.300288	0.000167	0.714386
-0.340821	-2.022216	0.305293	0.000190	0.714274
-0.089918	-2.127713	0.310298	0.000143	0.714153
-0.277835	-2.188642	0.315302	0.000178	0.713965
-0.159580	-2.251395	0.320307	0.000157	0.713882
-0.315938	-2.337501	0.325312	0.000186	0.713655
-0.632075	-2.308121	0.330317	0.000245	0.713601
-2.485032	-2.095547	0.335322	0.000590	0.713367
-2.616253	-2.077753	0.340326	0.000615	0.713356
-3.056826	-2.047494	0.345331	0.000697	0.713260
-3.756239	-2.041282	0.350336	0.000827	0.713024
-3.538126	-2.080355	0.355341	0.000787	0.713023
-3.797522	-2.036504	0.360346	0.000835	0.713018
-4.465904	-2.073179	0.365350	0.000960	0.712708
-4.292583	-2.099175	0.370355	0.000928	0.712717
-5.001236	-1.974608	0.375360	0.001060	0.712714
-4.969773	-2.042752	0.380365	0.001054	0.712589
-5.481592	-2.049938	0.385370	0.001149	0.712393
-5.414640	-2.065643	0.390374	0.001137	0.712385
-5.663664	-2.018190	0.395379	0.001184	0.712391
-5.752406	-2.032954	0.400384	0.001200	0.712329
-6.410906	-2.035272	0.405389	0.001323	0.712091
-6.172496	-2.075417	0.410394	0.001279	0.712095
-6.992891	-1.932969	0.415398	0.001432	0.712087
-6.402912	-2.035837	0.420403	0.001322	0.712092
-6.474235	-2.115018	0.425408	0.001335	0.711908
-7.951341	-1.925708	0.430413	0.001611	0.711761
-7.200821	-2.054290	0.435418	0.001471	0.711771
-7.390087	-2.025432	0.440422	0.001506	0.711761
-7.924257	-1.927678	0.445427	0.001606	0.711765
-7.702336	-2.018869	0.450432	0.001565	0.711662
-8.470195	-1.987490	0.455437	0.001708	0.711452
-7.984208	-2.069408	0.460442	0.001618	0.711461
-8.410457	-1.998710	0.465446	0.001697	0.711450
-8.212532	-2.028828	0.470451	0.001660	0.711460
-8.065091	-2.055193	0.475456	0.001633	0.711459
-8.904188	-2.062759	0.480461	0.001790	0.711146
-9.036908	-2.039631	0.485466	0.001814	0.711144
-9.358876	-1.987472	0.490470	0.001874	0.711134
-9.092201	-2.031056	0.495475	0.001825	0.711141
-9.161221	-2.018966	0.500480	0.001838	0.711141
-9.200225	-2.039251	0.505485	0.001845	0.711086
-9.542850	-2.082694	0.510490	0.001909	0.710877
-10.048125	-1.997398	0.515494	0.002004	0.710867
-10.189214	-1.969063	0.520499	0.002030	0.710873
-9.761781	-2.046067	0.525504	0.001951	0.710871
-10.241385	-1.962686	0.530509	0.002040	0.710867
-10.022031	-2.030680	0.535514	0.001999	0.710809
-10.842055	-2.021480	0.540518	0.002152	0.710535
-10.605198	-2.061319	0.545523	0.002108	0.710540
-11.041697	-1.986867	0.550528	0.002190	0.710533
-10.948767	-2.006294	0.555533	0.002172	0.710527
-10.456850	-2.087014	0.560538	0.002081	0.710540
-11.063504	-1.984428	0.565542	0.002194	0.710529
-11.262841	-2.100740	0.570547	0.002231	0.710225
-11.519556	-2.058324	0.575552	0.002279	0.710219
-12.248135	-1.931193	0.580557	0.002415	0.710213
-11.701327	-2.023809	0.585562	0.002313	0.710222
-11.862547	-2.000209	0.590566	0.002344	0.710212
-11.813802	-2.004847	0.595571	0.002335	0.710219
-11.834161	-2.066729	0.600576	0.002339	0.710088
-12.911559	-1.973836	0.605581	0.002539	0.709890
-12.170164	-2.101759	0.610586	0.002402	0.709898
-12.788082	-1.996883	0.615590	0.002517	0.709887
-12.865392	-1.979800	0.620595	0.002531	0.709894
-12.493141	-2.046036	0.625600	0.002462	0.709893
-13.001581	-1.956649	0.630605	0.002557	0.709891
-12.950927	-2.052934	0.635610	0.002548	0.709716
-13.789874	-1.967632	0.640614	0.002704	0.709587
-13.540385	-2.007738	0.645619	0.002658	0.709596
-13.613484	-1.994958	0.650624	0.002671	0.709595
-13.705228	-1.980845	0.655629	0.002689	0.709590
-13.088466	-2.085976	0.660634	0.002574	0.709599
-13.591941	-1.999656	0.665638	0.002668	0.709592
-14.016999	-2.051148	0.670643	0.002747	0.709337
-14.418223	-2.016672	0.675648	0.002822	0.709263
-14.358935	-2.027447	0.680653	0.002811	0.709262
-14.335839	-2.027246	0.685658	0.002807	0.709271
-14.657664	-1.973687	0.690662	0.002867	0.709263
-14.338298	-2.027653	0.695667	0.002808	0.709268
-14.215709	-2.049593	0.700672	0.002785	0.709268
-15.045578	-2.054023	0.705677	0.002940	0.708963
-15.086806	-2.045441	0.710682	0.002948	0.708965
-15.729993	-1.934525	0.715686	0.003067	0.708957
-15.475460	-1.978577	0.720691	0.003020	0.708960
-15.097489	-2.044589	0.725696	0.002950	0.708962
-15.411435	-1.991963	0.730701	0.003009	0.708955
-15.368058	-1.994600	0.735706	0.003001	0.708965
-15.925852	-2.043007	0.740710	0.003105	0.708669
-16.334904	-1.983715	0.745715	0.003181	0.708641
-16.474499	-1.957484	0.750720	0.003207	0.708644
-16.381844	-1.976934	0.755725	0.003190	0.708637
-16.102793	-2.022629	0.760730	0.003138	0.708645
-16.207948	-2.008304	0.765734	0.003158	0.708636
-16.116308	-2.021143	0.770739	0.003141	0.708643
-16.307316	-2.090637	0.775744	0.003177	0.708435
-17.341710	-1.948046	0.780749	0.003369	0.708351
-16.925188	-2.017662	0.785754	0.003292	0.708360
-16.878069	-2.030475	0.790758	0.003284	0.708351
-17.141956	-1.980611	0.795763	0.003333	0.708356
-17.154249	-1.980146	0.800768	0.003335	0.708353
-17.122305	-1.986164	0.805773	0.003329	0.708352
-17.356359	-2.096301	0.810778	0.003373	0.708047
-18.043171	-1.991886	0.815782	0.003501	0.708011
-18.401786	-1.924788	0.820787	0.003568	0.708017
-17.888256	-2.016720	0.825792	0.003473	0.708016
-18.094782	-1.981752	0.830797	0.003511	0.708012
-18.039147	-1.987632	0.835802	0.003501	0.708020
-18.140594	-1.973573	0.840806	0.003520	0.708011
-17.983099	-2.112286	0.845811	0.003491	0.707789
-18.943974	-1.983491	0.850816	0.003670	0.707704
-19.232633	-1.936372	0.855821	0.003724	0.707695
-18.449789	-2.070589	0.860826	0.003578	0.707705
-18.865658	-1.999629	0.865830	0.003656	0.707698
-19.007107	-1.971666	0.870835	0.003682	0.707704
-18.842510	-2.000394	0.875840	0.003652	0.707705
-19.380894	-2.040424	0.880845	0.003752	0.707431
-20.058288	-1.945173	0.885850	0.003878	0.707380
-19.870666	-1.983451	0.890854	0.003844	0.707370
-19.654988	-2.019262	0.895859	0.003804	0.707375
-19.942728	-1.965808	0.900864	0.003857	0.707379
-20.051403	-1.948940	0.905869	0.003878	0.707374
-19.697847	-2.007032	0.910874	0.003812	0.707383
-19.783848	-2.055266	0.915878	0.003828	0.707256
-20.862796	-1.949903	0.920883	0.004029	0.707081
-20.381685	-2.035673	0.925888	0.003940	0.707080
-20.634183	-1.992156	0.930893	0.003987	0.707077
-20.653181	-1.984661	0.935898	0.003991	0.707085
-20.572661	-2.002214	0.940902	0.003976	0.707078
-20.597685	-1.994656	0.945907	0.003981	0.707084
-20.573509	-2.102847	0.950912	0.003976	0.706875
-21.987676	-1.912807	0.955917	0.004240	0.706751
-21.619164	-1.974739	0.960922	0.004171	0.706758
-21.499565	-1.999023	0.965926	0.004149	0.706752
-22.057976	-1.900042	0.970931	0.004253	0.706750
-21.649839	-1.970435	0.975936	0.004177	0.706755
-21.472234	-2.005176	0.980941	0.004145	0.706748
-21.449528	-2.052523	0.985946	0.004141	0.706661
-22.528056	-1.969058	0.990950	0.004341	0.706442
-22.216279	-2.022549	0.995955	0.004284	0.706446
-22.371223	-1.993543	1.000960	0.004313	0.706448
-22.774653	-1.923933	1.005965	0.004388	0.706443
-22.447120	-1.978718	1.010970	0.004327	0.706450
-22.374472	-1.994749	1.015974	0.004314	0.706444
-22.810535	-1.941966	1.020979	0.004395	0.706394
-23.221807	-1.998130	1.025984	0.004472	0.706133
-23.221359	-2.001833	1.030989	0.004472	0.706125
-23.525071	-1.943473	1.035994	0.004528	0.706134
-23.521648	-1.947745	1.040998	0.004528	0.706126
-23.301369	-1.984307	1.046003	0.004487	0.706131
-23.089964	-2.021306	1.051008	0.004448	0.706132
-23.778335	-1.901754	1.056013	0.004576	0.706126
-23.847984	-2.004364	1.061018	0.004589	0.705894
-24.085003	-1.977610	1.066022	0.004634	0.705863
-24.472936	-1.908196	1.071027	0.004706	0.705863
-24.172390	-1.959340	1.076032	0.004650	0.705867
-24.268499	-1.945518	1.081037	0.004668	0.705860
-23.989774	-1.990637	1.086042	0.004616	0.705869
-24.552113	-1.896071	1.091046	0.004721	0.705858
-24.525611	-2.044600	1.096051	0.004717	0.705568
-24.971281	-1.985645	1.101056	0.004800	0.705527
-25.483775	-1.897127	1.106061	0.004895	0.705521
-24.876560	-2.000150	1.111066	0.004782	0.705531
-25.035894	-1.973543	1.116070	0.004812	0.705527
-25.257105	-1.933810	1.121075	0.004853	0.705527
-25.228074	-1.938648	1.126080	0.004848	0.705528
-25.571441	-2.019619	1.131085	0.004912	0.705241
-25.718779	-2.005346	1.136090	0.004940	0.705217
-26.114761	-1.939573	1.141094	0.005014	0.705207
-25.921457	-1.972495	1.146099	0.004978	0.705210
-25.784662	-1.994296	1.151104	0.004953	0.705214
-26.321739	-1.902246	1.156109	0.005053	0.705207
-26.169313	-1.924158	1.161114	0.005025	0.705217
-26.453162	-2.017843	1.166118	0.005078	0.704926
-26.964885	-1.944919	1.171123	0.005173	0.704889
-27.095769	-1.918614	1.176128	0.005197	0.704895
-26.647417	-2.002238	1.181133	0.005114	0.704887
-26.647633	-1.999460	1.186138	0.005114	0.704892
-27.252041	-1.895131	1.191142	0.005227	0.704885
-27.060856	-1.927754	1.196147	0.005192	0.704888
-26.891616	-2.060306	1.201152	0.005160	0.704681
-28.038785	-1.902597	1.206157	0.005374	0.704587
-27.816337	-1.937502	1.211162	0.005333	0.704596
-27.782675	-1.946188	1.216166	0.005327	0.704590
-27.810764	-1.940379	1.221171	0.005332	0.704591
-27.802427	-1.939399	1.226176	0.005331	0.704596
-27.645707	-1.970914	1.231181	0.005302	0.704589
-27.769780	-2.073666	1.236186	0.005325	0.704337
-28.752531	-1.936608	1.241190	0.005508	0.704260
-28.681965	-1.948116	1.246195	0.005495	0.704261
-28.246644	-2.023222	1.251200	0.005414	0.704266
-28.709444	-1.945680	1.256205	0.005500	0.704256
-28.635833	-1.954131	1.261210	0.005487	0.704265
-28.394424	-2.004345	1.266214	0.005442	0.704250
-29.085909	-2.027891	1.271219	0.005571	0.703954
-29.638870	-1.928002	1.276224	0.005674	0.703956
-29.651804	-1.928610	1.281229	0.005677	0.703950
-29.008605	-2.038381	1.286234	0.005557	0.703960
-29.530883	-1.950308	1.291238	0.005654	0.703949
-29.840470	-1.892029	1.296243	0.005712	0.703955
-29.317527	-1.994446	1.301248	0.005615	0.703936
-30.186532	-1.990062	1.306253	0.005777	0.703632
-30.346835	-1.956852	1.311258	0.005807	0.703641
-30.548148	-1.924800	1.316262	0.005844	0.703633
-29.897792	-2.036820	1.321267	0.005724	0.703641
-30.341471	-1.957302	1.326272	0.005806	0.703642
-30.890469	-1.862372	1.331277	0.005909	0.703635
-30.143714	-2.000281	1.336282	0.005770	0.703625
-30.897326	-2.004838	1.341286	0.005910	0.703345
-31.464645	-1.902965	1.346291	0.006016	0.703346
-31.373069	-1.918840	1.351296	0.005999	0.703347
-31.202890	-1.951166	1.356301	0.005968	0.703342
-31.287726	-1.930020	1.361306	0.005984	0.703354
-31.130996	-1.963505	1.366310	0.005955	0.703343
-30.945850	-2.011142	1.371315	0.005920	0.703313
-32.098172	-1.954744	1.376320	0.006135	0.703012
-32.346197	-1.914706	1.381325	0.006181	0.703003
-32.027974	-1.965158	1.386330	0.006122	0.703015
-32.000504	-1.973854	1.391334	0.006117	0.703007
-32.103125	-1.955646	1.396339	0.006136	0.703007
-31.826853	-2.001980	1.401344	0.006085	0.703012
-31.806320	-2.045183	1.406349	0.006082	0.702932
-32.792230	-1.983953	1.411354	0.006265	0.702701
-32.828716	-1.980858	1.416358	0.006272	0.702693
-32.873586	-1.972908	1.421363	0.006281	0.702693
-32.820683	-1.979224	1.426368	0.006271	0.702699
-32.992982	-1.951488	1.431373	0.006303	0.702693
-32.601955	-2.016586	1.436378	0.006231	0.702702
-32.847439	-2.067526	1.441382	0.006276	0.702510
-34.329276	-1.870038	1.446387	0.006552	0.702375
-33.598294	-1.998149	1.451392	0.006417	0.702379
-33.619237	-1.999059	1.456397	0.006421	0.702369
-33.990268	-1.928859	1.461402	0.006490	0.702377
-34.265276	-1.883773	1.466406	0.006541	0.702369
-33.842489	-1.958398	1.471411	0.006463	0.702370
-33.440653	-2.092135	1.476416	0.006388	0.702244
-34.978667	-1.902737	1.481421	0.006674	0.702073
-34.570910	-1.970362	1.486426	0.006599	0.702083
-34.736460	-1.944366	1.491430	0.006630	0.702075
-34.909536	-1.913554	1.496435	0.006662	0.702075
-34.573874	-1.970562	1.501440	0.006600	0.702080
-34.745492	-1.943715	1.506445	0.006632	0.702072
-34.770849	-2.012982	1.511450	0.006637	0.701923
-35.819327	-1.914800	1.516454	0.006832	0.701743
-35.227148	-2.019055	1.521459	0.006722	0.701745
-35.222457	-2.017974	1.526464	0.006721	0.701749
-35.766076	-1.923442	1.531469	0.006822	0.701744
-35.375865	-1.988174	1.536474	0.006750	0.701753
-35.540577	-1.962131	1.541478	0.006781	0.701746
-36.155499	-1.947827	1.546483	0.006895	0.701553
-36.692844	-1.907349	1.551488	0.006996	0.701441
-36.332321	-1.975234	1.556493	0.006929	0.701433
-36.144607	-2.003321	1.561498	0.006894	0.701444
-36.771855	-1.894836	1.566502	0.007011	0.701437
-36.684562	-1.909796	1.571507	0.006995	0.701437
-36.097278	-2.012912	1.576512	0.006886	0.701440
-36.558263	-1.990628	1.581517	0.006972	0.701319
-37.355915	-1.941826	1.586522	0.007120	0.701129
-37.007595	-2.008305	1.591526	0.007056	0.701120
-37.523575	-1.914802	1.596531	0.007152	0.701123
-37.196190	-1.969417	1.601536	0.007091	0.701130
-37.083091	-1.995261	1.606541	0.007070	0.701119
-37.022241	-2.002925	1.611546	0.007059	0.701125
-37.523575	-2.003236	1.616550	0.007152	0.700943
-38.069843	-1.940928	1.621555	0.007254	0.700871
-37.610742	-2.017223	1.626560	0.007169	0.700882
-37.959507	-1.958469	1.631565	0.007234	0.700875
-38.034693	-1.941721	1.636570	0.007248	0.700881
-37.936966	-1.961702	1.641574	0.007230	0.700876
-38.123647	-1.982079	1.646579	0.007265	0.700767
-38.975947	-1.941121	1.651584	0.007424	0.700542
-38.929421	-1.952702	1.656589	0.007415	0.700535
-38.919582	-1.950540	1.661594	0.007414	0.700542
-39.103152	-1.920164	1.666598	0.007448	0.700537
-38.994550	-1.939157	1.671603	0.007428	0.700538
-38.571292	-2.014301	1.676608	0.007349	0.700538
-39.252855	-1.949939	1.681613	0.007476	0.700422
-39.980420	-1.916079	1.686618	0.007612	0.700227
-39.773223	-1.956581	1.691622	0.007573	0.700220
-39.942710	-1.924866	1.696627	0.007605	0.700222
-39.502596	-2.001286	1.701632	0.007523	0.700226
-39.737749	-1.964133	1.706637	0.007567	0.700216
-39.708391	-1.964146	1.711642	0.007562	0.700227
-39.995760	-1.985713	1.716646	0.007616	0.700079
-40.762876	-1.939286	1.721651	0.007759	0.699895
-40.097910	-2.054538	1.726656	0.007635	0.699901
-40.932943	-1.909593	1.731661	0.007791	0.699893
-40.756803	-1.935709	1.736666	0.007758	0.699904
-40.491873	-1.987005	1.741670	0.007709	0.699895
-40.840681	-1.923464	1.746675	0.007774	0.699897
-40.976100	-1.980707	1.751680	0.007799	0.699732
-42.042730	-1.857169	1.756685	0.007998	0.699596
-41.365618	-1.975207	1.761690	0.007872	0.699602
-41.639908	-1.925647	1.766694	0.007923	0.699603
-41.690446	-1.918760	1.771699	0.007933	0.699598
-41.117559	-2.017748	1.776704	0.007826	0.699604
-41.632183	-1.929595	1.781709	0.007922	0.699597
-41.785124	-1.988365	1.786714	0.007951	0.699422
-42.658880	-1.908144	1.791718	0.008114	0.699268
-42.275470	-1.977841	1.796723	0.008042	0.699265
-42.496875	-1.935137	1.801728	0.008084	0.699271
-42.575971	-1.925768	1.806733	0.008099	0.699261
-42.129716	-2.001523	1.811738	0.008016	0.699269
-42.341637	-1.966160	1.816742	0.008055	0.699263
-42.983611	-1.951384	1.821747	0.008175	0.699060
-43.281012	-1.947601	1.826752	0.008231	0.698960
-43.330935	-1.942549	1.831757	0.008240	0.698952
-43.133186	-1.972719	1.836762	0.008203	0.698962
-43.255484	-1.952109	1.841766	0.008226	0.698959
-43.237584	-1.956886	1.846771	0.008223	0.698956
-43.254960	-1.952377	1.851776	0.008226	0.698958
-43.559163	-2.013039	1.856781	0.008283	0.698725
-44.243671	-1.932126	1.861786	0.008411	0.698641
-44.237165	-1.935715	1.866790	0.008410	0.698635
-44.426375	-1.899638	1.871795	0.008445	0.698640
-44.138827	-1.948169	1.876800	0.008392	0.698645
-44.418176	-1.903387	1.881805	0.008444	0.698635
-44.196823	-1.939229	1.886810	0.008403	0.698642
-44.205723	-2.004027	1.891814	0.008405	0.698506
-44.922353	-1.954365	1.896819	0.008538	0.698347
-44.720693	-1.986928	1.901824	0.008501	0.698354
-45.138842	-1.915544	1.906829	0.008579	0.698347
-44.741925	-1.981895	1.911834	0.008505	0.698356
-44.916601	-1.953514	1.916838	0.008538	0.698350
-45.205630	-1.903356	1.921843	0.008592	0.698347
-45.251359	-2.048717	1.926848	0.008601	0.698034
-45.607944	-1.999204	1.931853	0.008667	0.698005
-45.892373	-1.944149	1.936858	0.008720	0.698014
-45.878689	-1.949630	1.941862	0.008718	0.698007
-45.948623	-1.938280	1.946867	0.008731	0.698005
-45.839553	-1.954062	1.951872	0.008711	0.698012
-46.042456	-1.952286	1.956877	0.008749	0.697941
-46.649718	-1.961705	1.961882	0.008862	0.697702
-46.547496	-1.982172	1.966886	0.008843	0.697697
-47.022574	-1.897982	1.971891	0.008932	0.697695
-46.493104	-1.989402	1.976896	0.008833	0.697701
-46.692775	-1.958514	1.981901	0.008870	0.697691
-47.129782	-1.877319	1.986906	0.008952	0.697698
-46.898830	-1.932976	1.991910	0.008909	0.697668
-47.427123	-1.985477	1.996915	0.009008	0.697369
-47.654043	-1.942426	2.001920	0.009050	0.697374
-47.431513	-1.981027	2.011917	0.009009	0.697375
-47.720517	-1.929806	2.021914	0.009063	0.697374
-47.450551	-1.978134	2.031910	0.009013	0.697373
-47.496521	-1.970647	2.041907	0.009022	0.697371
-47.608049	-1.948780	2.051904	0.009043	0.697375
-47.825742	-1.970320	2.061901	0.009084	0.697251
-47.582263	-1.953575	2.071898	0.009039	0.697373
-47.658513	-1.939842	2.081894	0.009053	0.697373
-47.621189	-1.945677	2.091891	0.009047	0.697374
-47.452336	-1.974780	2.101888	0.009016	0.697375
-47.417580	-1.979735	2.111885	0.009009	0.697377
-47.467043	-1.971010	2.121882	0.009019	0.697376
-47.427015	-1.979322	2.131878	0.009012	0.697373
-47.456640	-1.972793	2.141875	0.009018	0.697375
-46.847901	-1.959702	2.151872	0.008904	0.697623
-46.526474	-1.978515	2.161869	0.008845	0.697700
-46.592673	-1.965923	2.171866	0.008858	0.697701
-46.598365	-1.965505	2.181862	0.008859	0.697700
-46.687025	-1.934319	2.191859	0.008876	0.697730
-45.859136	-1.944465	2.201856	0.008722	0.698010
-45.638871	-1.982198	2.211853	0.008681	0.698012
-45.637557	-1.980611	2.221850	0.008681	0.698015
-45.566280	-1.994920	2.231846	0.008668	0.698012
-45.149281	-1.914966	2.241843	0.008591	0.698325
-44.949146	-1.938541	2.251840	0.008554	0.698349
-44.745287	-1.973309	2.261837	0.008516	0.698352
-44.900797	-1.921962	2.271834	0.008545	0.698399
-43.870770	-1.988813	2.281830	0.008354	0.698636
-43.951966	-1.972970	2.291827	0.008369	0.698638
-44.008405	-1.960811	2.301824	0.008380	0.698642
-43.730298	-1.937155	2.311821	0.008329	0.698790
-43.338164	-1.921782	2.321818	0.008256	0.698963
-43.130691	-1.960306	2.331814	0.008218	0.698959
-43.431207	-1.895001	2.341811	0.008274	0.698983
-42.298395	-1.955026	2.351808	0.008063	0.699271
-42.377669	-1.941218	2.361805	0.008078	0.699269
-42.449247	-1.928360	2.371802	0.008092	0.699269
-41.935526	-1.909743	2.381798	0.007997	0.699492
-41.784072	-1.884270	2.391795	0.007969	0.699598
-41.475653	-1.939527	2.401792	0.007912	0.699597
-41.442426	-1.904589	2.411789	0.007906	0.699679
-40.666427	-1.934641	2.421786	0.007761	0.699899
-40.515448	-1.962552	2.431782	0.007734	0.699896
-41.024635	-1.872345	2.441779	0.007829	0.699894
-40.008643	-1.910715	2.451776	0.007640	0.700184
-40.006658	-1.892905	2.461773	0.007640	0.700220
-39.770815	-1.935256	2.471770	0.007596	0.700219
-39.520845	-1.893532	2.481766	0.007550	0.700393
-38.883468	-1.938451	2.491763	0.007432	0.700532
-38.856416	-1.941872	2.501760	0.007427	0.700534
-38.769523	-1.956542	2.511757	0.007411	0.700535
-38.252146	-1.907200	2.521754	0.007315	0.700822
-37.993551	-1.927534	2.531750	0.007267	0.700873
-37.946869	-1.937232	2.541747	0.007259	0.700870
-37.842469	-1.919074	2.551744	0.007240	0.700944
-37.323565	-1.923938	2.561741	0.007143	0.701121
-37.136473	-1.957015	2.571738	0.007109	0.701121
-37.416248	-1.908344	2.581734	0.007161	0.701118
-36.656474	-1.891215	2.591731	0.007020	0.701426
-36.349790	-1.941486	2.601728	0.006963	0.701435
-36.397619	-1.933830	2.611725	0.006972	0.701432
-35.835070	-1.934440	2.621722	0.006868	0.701634
-35.758138	-1.893769	2.631718	0.006854	0.701743
-35.506088	-1.938660	2.641715	0.006807	0.701743
-35.373381	-1.924265	2.651712	0.006783	0.701819
-34.815574	-1.897425	2.661709	0.006679	0.702074
-34.429832	-1.967853	2.671706	0.006608	0.702070
-34.754855	-1.909304	2.681702	0.006668	0.702071
-34.011785	-1.922677	2.691699	0.006530	0.702311
-33.836252	-1.925936	2.701696	0.006498	0.702367
-33.961945	-1.903896	2.711693	0.006522	0.702366
-33.491107	-1.913451	2.721690	0.006434	0.702516
-33.033969	-1.907977	2.731686	0.006350	0.702691
-32.957920	-1.921367	2.741683	0.006336	0.702690
-32.925937	-1.926630	2.751680	0.006330	0.702691
-32.018730	-1.931739	2.761677	0.006161	0.703007
-31.969931	-1.940231	2.771674	0.006153	0.703007
-32.109789	-1.914622	2.781670	0.006179	0.703007
-31.873339	-1.885912	2.791667	0.006135	0.703150
-31.065837	-1.934033	2.801664	0.005985	0.703343
-31.000434	-1.944131	2.811661	0.005973	0.703345
-30.983740	-1.946706	2.821658	0.005971	0.703346
-30.561488	-1.908838	2.831654	0.005892	0.703573
-30.142387	-1.952835	2.841651	0.005814	0.703635
-30.322223	-1.920408	2.851648	0.005848	0.703635
-30.074364	-1.920275	2.861645	0.005802	0.703724
-29.395219	-1.927717	2.871642	0.005676	0.703953
-29.453931	-1.919366	2.881638	0.005687	0.703948
-29.555652	-1.899240	2.891635	0.005707	0.703951
-28.755889	-1.899423	2.901632	0.005558	0.704238
-28.517432	-1.929750	2.911629	0.005514	0.704262
-28.484009	-1.935811	2.921626	0.005508	0.704261
-28.387042	-1.882252	2.931622	0.005490	0.704403
-27.437492	-1.959192	2.941619	0.005314	0.704589
-27.761949	-1.901411	2.951616	0.005374	0.704588
-27.382842	-1.967627	2.961613	0.005304	0.704590
-26.864599	-1.936025	2.971610	0.005208	0.704839
-26.894065	-1.908138	2.981606	0.005214	0.704884
-26.641430	-1.951455	2.991603	0.005167	0.704887
-26.556655	-1.921154	3.001600	0.005152	0.704978
-25.550683	-1.983376	3.011597	0.004965	0.705213
-25.873971	-1.925963	3.021594	0.005025	0.705212
-25.656423	-1.964887	3.031590	0.004985	0.705212
-25.286993	-1.938248	3.041587	0.004916	0.705397
-24.952566	-1.935096	3.051584	0.004854	0.705523
-24.778920	-1.963979	3.061581	0.004822	0.705526
-24.887893	-1.941277	3.071578	0.004843	0.705532
-24.105687	-1.917579	3.081574	0.004698	0.705860
-23.951116	-1.944382	3.091571	0.004669	0.705861
-23.941809	-1.945212	3.101568	0.004668	0.705862
-23.736815	-1.927491	3.111565	0.004630	0.705971
-23.146544	-1.953641	3.121562	0.004520	0.706129
-23.145046	-1.954089	3.131558	0.004520	0.706128
-23.167884	-1.950665	3.141555	0.004525	0.706126
-22.558525	-1.908920	3.151552	0.004412	0.706428
-22.175559	-1.967644	3.161549	0.004341	0.706447
-22.235009	-1.956139	3.171546	0.004352	0.706448
-22.124089	-1.904836	3.181542	0.004332	0.706590
-21.411696	-1.950615	3.191539	0.004199	0.706753
-21.494115	-1.934666	3.201536	0.004215	0.706755
-21.353821	-1.949777	3.211533	0.004189	0.706774
-20.722963	-1.907666	3.221530	0.004072	0.707084
-20.439627	-1.959442	3.231526	0.004019	0.707080
-20.674849	-1.917423	3.241523	0.004064	0.707080
-20.186417	-1.913758	3.251520	0.003973	0.707262
-19.626817	-1.955078	3.261517	0.003869	0.707378
-19.776610	-1.927508	3.271514	0.003897	0.707379
-19.574313	-1.939290	3.281510	0.003860	0.707428
-18.900518	-1.924744	3.291507	0.003735	0.707697
-18.735073	-1.952818	3.301504	0.003704	0.707699
-18.883855	-1.925624	3.311501	0.003732	0.707700
-18.381610	-1.905469	3.321498	0.003639	0.707920
-17.843402	-1.955273	3.331494	0.003539	0.708011
-17.780281	-1.967252	3.341491	0.003528	0.708009
-17.825293	-1.944754	3.351488	0.003536	0.708038
-17.194153	-1.901458	3.361485	0.003419	0.708350
-17.060572	-1.922173	3.371482	0.003394	0.708355
-16.981240	-1.936963	3.381478	0.003380	0.708353
-16.786481	-1.876798	3.391475	0.003344	0.708543
-15.991243	-1.971508	3.401472	0.003196	0.708636
-16.233227	-1.926533	3.411469	0.003242	0.708640
-15.979472	-1.955476	3.421466	0.003195	0.708672
-15.409904	-1.914250	3.431462	0.003089	0.708957
-15.318811	-1.931645	3.441459	0.003072	0.708954
-15.066231	-1.974150	3.451456	0.003025	0.708958
-14.913373	-1.917052	3.461453	0.002997	0.709127
-14.231766	-1.967524	3.471450	0.002871	0.709268
-14.450532	-1.929187	3.481446	0.002912	0.709266
-14.522181	-1.908985	3.491443	0.002925	0.709281
-13.568184	-1.921722	3.501440	0.002748	0.709595
-13.252010	-1.976690	3.511437	0.002689	0.709597
-13.157277	-1.994225	3.521434	0.002672	0.709595
-13.194340	-1.947712	3.531430	0.002679	0.709674
-12.467968	-1.967324	3.541427	0.002544	0.709893
-12.080026	-2.036957	3.551424	0.002472	0.709892
-12.451026	-1.969264	3.561421	0.002542	0.709894
-12.097576	-1.958900	3.571418	0.002476	0.710040
-11.289645	-2.014494	3.581414	0.002326	0.710216
-11.272218	-2.018566	3.591411	0.002323	0.710214
-11.323082	-2.008629	3.601408	0.002333	0.710215
-11.092547	-1.961225	3.611405	0.002290	0.710391
-10.294342	-2.032410	3.621402	0.002142	0.710533
-10.587289	-1.980702	3.631398	0.002197	0.710531
-10.515598	-1.993232	3.641395	0.002184	0.710531
-9.775086	-1.976661	3.651392	0.002046	0.710827
-9.533655	-1.996577	3.661389	0.002002	0.710873
-9.351993	-2.029016	3.671386	0.001968	0.710872
-9.514296	-1.995698	3.681382	0.001999	0.710880
-8.848900	-1.986419	3.691379	0.001875	0.711135
-8.710575	-2.010587	3.701376	0.001850	0.711135
-8.650673	-2.019135	3.711373	0.001839	0.711139
-8.565065	-1.954987	3.721370	0.001823	0.711297
-8.061454	-1.965464	3.731366	0.001730	0.711454
-8.009091	-1.976037	3.741363	0.001720	0.711451
-7.852988	-1.975279	3.751360	0.001691	0.711508
-7.034182	-1.993174	3.761357	0.001539	0.711762
-6.795688	-2.035464	3.771354	0.001495	0.711762
-7.069860	-1.987304	3.781350	0.001546	0.711760
-6.357444	-2.011600	3.791347	0.001414	0.711964
-6.023512	-2.007604	3.801344	0.001352	0.712090
-6.136891	-1.986450	3.811341	0.001374	0.712092
-5.747003	-2.056892	3.821338	0.001301	0.712089
-5.811740	-1.920533	3.831334	0.001314	0.712337
-5.107367	-2.022176	3.841331	0.001183	0.712384
-5.067475	-2.027822	3.851328	0.001176	0.712387
-4.913649	-2.000365	3.861325	0.001147	0.712495
-3.953454	-2.062844	3.871322	0.000969	0.712711
-4.219130	-2.016477	3.881318	0.001019	0.712708
-4.159288	-2.028503	3.891315	0.001008	0.712705
-3.767576	-1.996056	3.901312	0.000935	0.712908
-3.234032	-2.033033	3.911309	0.000836	0.713023
-3.081455	-2.060364	3.921306	0.000808	0.713022
-3.243730	-2.031048	3.931302	0.000838	0.713023
-2.425052	-2.027993	3.941299	0.000686	0.713318
-2.460637	-2.000897	3.951296	0.000693	0.713359
-2.372524	-2.014150	3.961293	0.000677	0.713363
-2.265870	-1.992631	3.971290	0.000658	0.713443
-1.530283	-2.017799	3.981286	0.000521	0.713653
-1.504972	-2.023989	3.991283	0.000517	0.713649
-1.669397	-1.993229	4.001280	0.000547	0.713652
-1.263899	-1.936276	4.011277	0.000472	0.713908
-1.271727	-1.900895	4.021274	0.000474	0.713975
-1.150522	-1.924878	4.031270	0.000452	0.713970
-0.875460	-1.841360	4.041267	0.000401	0.714232
-0.677916	-1.851877	4.051264	0.000364	0.714281
-0.827331	-1.791490	4.061261	0.000392	0.714347
-0.934503	-1.638425	4.071258	0.000412	0.714613
-0.763711	-1.660183	4.081254	0.000381	0.714629
-0.614984	-1.544661	4.091251	0.000353	0.714911
-0.542069	-1.551026	4.101248	0.000340	0.714923
-0.533897	-1.395159	4.111245	0.000339	0.715235
-0.620709	-1.339655	4.121242	0.000355	0.715314
-0.424607	-1.255651	4.131238	0.000319	0.715549
-0.525259	-1.137035	4.141235	0.000338	0.715748
-0.483436	-1.064870	4.151232	0.000330	0.715905
-0.262482	-0.987875	4.161229	0.000290	0.716135
-0.119926	-0.920668	4.171226	0.000263	0.716318
-0.415750	-0.768876	4.181222	0.000319	0.716514
-0.502804	-0.631072	4.191219	0.000335	0.716756
-0.410508	-0.491012	4.201216	0.000318	0.717065
-0.212884	-0.407536	4.211213	0.000281	0.717299
-0.066668	-0.306683	4.221210	0.000254	0.717549
0.117175	-0.205053	4.231206	0.000220	0.717814
-0.016709	-0.044606	4.241203	0.000246	0.718084
-0.131198	0.132578	4.251200	0.000267	0.718393
0.000000	0.293710	4.261197	0.000243	0.718757
-0.051015	0.919609	4.266202	0.000252	0.719973
0.222236	2.115592	4.271206	0.000201	0.722421
0.373597	3.938064	4.276211	0.000171	0.726044
0.825582	6.256863	4.281216	0.000086	0.730717
1.272607	9.097379	4.286221	0.000001	0.736365
1.601914	12.424448	4.291226	-0.000062	0.742859
1.863538	16.225561	4.296230	-0.000114	0.750171
2.157014	20.426846	4.301235	-0.000171	0.758172
2.412107	25.017097	4.306240	-0.000221	0.766797
3.001011	29.936072	4.311245	-0.000334	0.776035
3.431879	35.211219	4.316250	-0.000417	0.785757
4.076530	40.792492	4.321254	-0.000541	0.795973
4.464496	46.703638	4.326259	-0.000617	0.806560
4.833375	52.910524	4.331264	-0.000689	0.817518
5.192684	59.387307	4.336269	-0.000760	0.828789
5.703279	66.064214	4.341274	-0.000860	0.840292
6.829915	72.855028	4.346278	-0.001074	0.852009
7.230639	79.988201	4.351283	-0.001153	0.863920
7.898636	87.263988	4.356288	-0.001282	0.875975
8.228169	94.771562	4.361293	-0.001348	0.888141
8.590876	102.429363	4.366298	-0.001420	0.900389
9.110607	110.203934	4.371302	-0.001522	0.912697
15.826851	117.042463	4.376307	-0.002777	0.925070
19.191547	124.714204	4.381312	-0.003408	0.937648
19.404223	133.047626	4.386317	-0.003453	0.950224
19.722588	141.413268	4.391322	-0.003518	0.962709
20.251068	149.832043	4.396326	-0.003621	0.975165
20.916140	158.280458	4.401331	-0.003751	0.987540
21.725800	166.758123	4.406336	-0.003907	0.999839
22.913539	175.208470	4.411341	-0.004133	1.012042
23.620479	183.784151	4.416346	-0.004270	1.024157
24.350201	192.394900	4.421350	-0.004412	1.036183
25.467003	200.958086	4.426355	-0.004625	1.048096
26.433103	209.578903	4.431360	-0.004810	1.059918
27.347773	218.236973	4.436365	-0.004986	1.071646
28.088321	226.892675	4.441370	-0.005130	1.083204
28.978855	235.545369	4.446374	-0.005301	1.094670
30.128673	244.156125	4.451379	-0.005520	1.106019
30.592176	252.893353	4.456384	-0.005612	1.117263
31.592665	261.527451	4.461389	-0.005804	1.128382
31.955795	270.264746	4.466394	-0.005877	1.139383
32.576544	278.970255	4.471398	-0.005998	1.150295
33.701974	287.560676	4.476403	-0.006213	1.161068
34.526296	296.181350	4.481408	-0.006372	1.171716
35.118138	304.839167	4.486413	-0.006488	1.182265
35.563179	313.495750	4.491418	-0.006576	1.192689
36.507469	322.055649	4.496422	-0.006758	1.203008
37.403356	330.628166	4.501427	-0.006930	1.213245
37.851420	339.246342	4.506432	-0.007019	1.223360
38.649619	347.832296	4.511437	-0.007173	1.233423
39.597999	356.329656	4.516442	-0.007355	1.243333
40.293992	364.882739	4.521446	-0.007490	1.253178
40.765425	373.442788	4.526451	-0.007583	1.262912
41.282078	381.982717	4.531456	-0.007685	1.272556
41.723599	390.514675	4.536461	-0.007772	1.282106
42.353177	398.998428	4.541466	-0.007895	1.291566
43.178063	407.434528	4.546470	-0.008054	1.300941
44.172187	415.909779	4.551475	-0.008244	1.310322
44.702478	424.442624	4.556480	-0.008348	1.319614
45.636874	432.823082	4.561485	-0.008528	1.328750
46.315812	441.239848	4.566490	-0.008659	1.337817
46.696460	449.682264	4.571494	-0.008736	1.346797
47.399213	458.080732	4.576499	-0.008872	1.355727
48.109317	466.437449	4.581504	-0.009009	1.364557
48.501279	474.882022	4.586509	-0.009088	1.373365
48.912416	483.265362	4.591514	-0.009170	1.382058
49.574922	491.636719	4.596518	-0.009298	1.390727
50.172973	499.997774	4.601523	-0.009415	1.399320
50.652489	508.345221	4.606528	-0.009509	1.407827
51.606882	516.649624	4.611533	-0.009692	1.416318
52.185561	524.974947	4.616538	-0.009805	1.424718
52.877773	533.311520	4.621542	-0.009940	1.433097
53.356769	541.637171	4.626547	-0.010034	1.441383
53.889049	549.949681	4.631552	-0.010138	1.449616
54.400884	558.290659	4.636557	-0.010239	1.457827
54.952398	566.573754	4.641562	-0.010347	1.465943
55.614102	574.913267	4.646566	-0.010476	1.474085
56.362152	583.159307	4.651571	-0.010620	1.482106
56.549658	591.493701	4.656576	-0.010660	1.490081
57.749034	599.682290	4.661581	-0.010889	1.498031
58.566470	607.907976	4.666586	-0.011046	1.505915
59.065227	616.220325	4.671590	-0.011144	1.513791
59.403688	624.515076	4.676595	-0.011213	1.521585
59.954468	632.768612	4.681600	-0.011320	1.529332
60.388585	641.058975	4.686605	-0.011406	1.537057
60.781840	649.319464	4.691610	-0.011485	1.544710
61.270538	657.594027	4.696614	-0.011581	1.552352
61.788753	665.827718	4.701619	-0.011683	1.559923
62.232082	674.050114	4.706624	-0.011771	1.567436
62.992654	682.265337	4.711629	-0.011917	1.574953
63.361077	690.508476	4.716634	-0.011991	1.582403
63.678643	698.771281	4.721638	-0.012056	1.589827
63.948805	707.035528	4.726643	-0.012111	1.597212
64.801615	715.173904	4.731648	-0.012275	1.604534
65.394392	723.395390	4.736653	-0.012391	1.611858
65.759166	731.630503	4.741658	-0.012464	1.619130
66.295048	739.834496	4.746662	-0.012569	1.626365
66.708764	748.110684	4.751667	-0.012651	1.633614
67.050222	756.299690	4.756672	-0.012720	1.640745
67.475755	764.497727	4.761677	-0.012804	1.647865
67.820112	772.703436	4.766682	-0.012874	1.654949
68.445778	780.850907	4.771686	-0.012995	1.661992
69.113482	789.013369	4.776691	-0.013125	1.669023
69.765171	797.187323	4.781696	-0.013251	1.676032
70.245334	805.364786	4.786701	-0.013346	1.682992
70.774519	813.534437	4.791706	-0.013450	1.689922
71.485458	821.709508	4.796710	-0.013587	1.696853
71.993855	829.894041	4.801715	-0.013687	1.703737
72.015045	838.140954	4.806720	-0.013696	1.710580
72.574472	846.324687	4.811725	-0.013805	1.717415
72.855721	854.498511	4.816730	-0.013863	1.724177
73.083269	862.695061	4.821734	-0.013911	1.730925
73.546631	870.857007	4.826739	-0.014002	1.737649
73.992506	878.999971	4.831744	-0.014090	1.744329
74.367003	887.186379	4.836749	-0.014165	1.751010
74.688263	895.350970	4.841754	-0.014230	1.757640
75.212167	903.483624	4.846758	-0.014333	1.764246
75.955231	911.613159	4.851763	-0.014476	1.770851
76.332962	919.790499	4.856768	-0.014552	1.777424
76.948577	927.929682	4.861773	-0.014672	1.783972
77.228940	936.130125	4.866778	-0.014729	1.790504
77.883563	944.299625	4.871782	-0.014856	1.797032
78.435571	952.402452	4.876787	-0.014964	1.803473
78.909162	960.527371	4.881792	-0.015057	1.809897
79.243514	968.701343	4.886797	-0.015125	1.816321
79.603319	976.828330	4.891802	-0.015197	1.822688
79.996581	984.977134	4.896806	-0.015275	1.829054
80.292398	993.152113	4.901811	-0.015336	1.835406
80.684058	1001.268501	4.906816	-0.015414	1.841702
81.270170	1009.389943	4.911821	-0.015528	1.848004
81.664571	1017.538797	4.916826	-0.015606	1.854282
82.249023	1025.644315	4.921830	-0.015720	1.860529
82.568204	1033.811390	4.926835	-0.015785	1.866770
82.940867	1041.960365	4.931840	-0.015860	1.872983
83.579606	1050.075893	4.936845	-0.015984	1.879180
83.649837	1058.218894	4.941850	-0.016002	1.885313
84.172635	1066.349506	4.946854	-0.016104	1.891468
84.813912	1074.447044	4.951859	-0.016229	1.897591
85.250908	1082.550258	4.956864	-0.016315	1.903676
85.725654	1090.691360	4.961869	-0.016409	1.909773
86.314517	1098.786735	4.966874	-0.016524	1.915830
86.625896	1106.926242	4.971878	-0.016587	1.921870
87.130673	1115.035258	4.976883	-0.016686	1.927889
87.744495	1123.140214	4.981888	-0.016805	1.933899
88.305730	1131.263876	4.986893	-0.016915	1.939897
88.373795	1139.434302	4.991898	-0.016933	1.945857
88.933853	1147.580130	4.996902	-0.017042	1.951835
89.211636	1155.735447	5.001907	-0.017099	1.957770
89.123553	1163.868324	5.006912	-0.017088	1.963632
89.813492	1171.925218	5.011917	-0.017222	1.969505
90.279198	1180.033052	5.016922	-0.017313	1.975373
90.610664	1188.139101	5.021926	-0.017380	1.981208
91.060950	1196.240040	5.026931	-0.017469	1.987035
91.373693	1204.360552	5.031936	-0.017533	1.992844
91.892457	1212.453503	5.036941	-0.017634	1.998638
92.125526	1220.556387	5.041946	-0.017683	2.004393
92.435545	1228.674698	5.046950	-0.017746	2.010149
92.867324	1236.786317	5.051955	-0.017831	2.015897
93.355888	1244.847520	5.056960	-0.017927	2.021600
93.633168	1252.983864	5.061965	-0.017984	2.027316
94.086343	1261.105172	5.066970	-0.018074	2.033024
94.591380	1269.190569	5.071974	-0.018173	2.038697
94.880861	1277.291572	5.076979	-0.018232	2.044342
95.184325	1285.383094	5.081984	-0.018294	2.049967
96.089580	1293.434992	5.086989	-0.018467	2.055609
96.598223	1301.511636	5.091994	-0.018567	2.061213
96.935217	1309.636452	5.096998	-0.018635	2.066818
97.279301	1317.765656	5.102003	-0.018704	2.072411
97.502825	1325.882421	5.107008	-0.018751	2.077968
97.760555	1333.983034	5.112013	-0.018804	2.083503
97.993097	1342.090403	5.117018	-0.018852	2.089025
98.331664	1350.207268	5.122022	-0.018921	2.094549
98.882531	1358.259935	5.127027	-0.019028	2.100037
99.321019	1366.335510	5.132032	-0.019115	2.105514
99.697055	1374.478988	5.137037	-0.019190	2.111016
99.858018	1382.625341	5.142042	-0.019225	2.116485
100.209388	1390.680718	5.147046	-0.019296	2.121898
100.538707	1398.760123	5.152051	-0.019362	2.127311
101.036685	1406.822710	5.157056	-0.019460	2.132714
101.522097	1414.912191	5.162061	-0.019556	2.138121
101.987458	1422.967234	5.167066	-0.019647	2.143489
102.580513	1431.036168	5.172070	-0.019763	2.148865
102.763929	1439.184346	5.177075	-0.019802	2.154240
103.008887	1447.264190	5.182080	-0.019853	2.159564
103.450669	1455.338012	5.187085	-0.019940	2.164888
103.750986	1463.423231	5.192090	-0.020001	2.170194
103.906147	1471.558236	5.197094	-0.020035	2.175506
104.279978	1479.618441	5.202099	-0.020110	2.180776
104.689197	1487.671227	5.207104	-0.020191	2.186032
105.220303	1495.763438	5.212109	-0.020295	2.191312
105.588533	1503.861768	5.217114	-0.020369	2.196568
105.946108	1511.914722	5.222118	-0.020441	2.201781
106.496534	1519.977372	5.227123	-0.020548	2.207005
106.803022	1528.071440	5.232128	-0.020611	2.212216
107.433207	1536.136368	5.237133	-0.020733	2.217424
107.592792	1544.227470	5.242138	-0.020768	2.222594
107.758743	1552.326080	5.247142	-0.020804	2.227758
108.333649	1560.402603	5.252147	-0.020916	2.232932
108.309561	1568.517106	5.257152	-0.020917	2.238065
108.597368	1576.596777	5.262157	-0.020975	2.243192
108.814092	1584.670829	5.267162	-0.021021	2.248297
109.381449	1592.716560	5.272166	-0.021132	2.253404
109.626983	1600.811755	5.277171	-0.021182	2.258502
109.615720	1608.910883	5.282176	-0.021185	2.263568
109.885949	1617.005148	5.287181	-0.021241	2.268644
110.224494	1625.135634	5.292186	-0.021309	2.273738
110.893210	1633.126043	5.297190	-0.021439	2.278761
111.428887	1641.164021	5.302195	-0.021544	2.283791
111.546208	1649.238139	5.307200	-0.021570	2.288797
112.142700	1657.309611	5.312205	-0.021687	2.293831
112.305941	1665.383213	5.317210	-0.021722	2.298818
112.651025	1673.438320	5.322214	-0.021792	2.303798
113.175557	1681.503831	5.327219	-0.021894	2.308789
113.295356	1689.616534	5.332224	-0.021922	2.313764
113.896880	1697.651766	5.337229	-0.022039	2.318722
114.357095	1705.696727	5.342234	-0.022130	2.323662
114.543690	1713.782301	5.347238	-0.022169	2.328594
114.947189	1721.873144	5.352243	-0.022250	2.333537
115.105959	1729.953787	5.357248	-0.022284	2.338443
115.658650	1737.996243	5.362253	-0.022392	2.343348
115.835747	1746.091549	5.367258	-0.022431	2.348244
116.580924	1754.133751	5.372262	-0.022574	2.353143
117.007701	1762.203988	5.377267	-0.022659	2.358024
117.135565	1770.265340	5.382272	-0.022688	2.362864
117.715972	1778.308210	5.387277	-0.022801	2.367720
118.085062	1786.396688	5.392282	-0.022875	2.372577
118.394207	1794.465179	5.397286	-0.022938	2.377406
118.567396	1802.563539	5.402291	-0.022975	2.382233
119.027169	1810.592634	5.407296	-0.023066	2.387031
119.243720	1818.704790	5.412301	-0.023111	2.391850
119.481706	1826.770814	5.417306	-0.023160	2.396633
119.906830	1834.802451	5.422310	-0.023245	2.401402
120.001843	1842.898819	5.427315	-0.023268	2.406173
120.143239	1850.971631	5.432320	-0.023299	2.410924
120.716951	1859.020396	5.437325	-0.023411	2.415685
121.027254	1867.068791	5.442330	-0.023474	2.420416
121.244381	1875.132633	5.447334	-0.023519	2.425140
121.396611	1883.249895	5.452339	-0.023553	2.429881
121.849589	1891.358200	5.457344	-0.023642	2.434630
122.226336	1899.367754	5.462349	-0.023718	2.439307
122.271519	1907.425239	5.467354	-0.023731	2.443977
122.708229	1915.447533	5.472358	-0.023817	2.448648
123.283742	1923.501885	5.477363	-0.023930	2.453338
123.580095	1931.531279	5.482368	-0.023990	2.457984
123.959195	1939.590793	5.487373	-0.024066	2.462645
124.258101	1947.658055	5.492378	-0.024126	2.467296
124.332980	1955.760683	5.497382	-0.024145	2.471941
124.858200	1963.809294	5.502387	-0.024248	2.476580
125.208114	1971.835331	5.507392	-0.024319	2.481184
125.654640	1979.889757	5.512397	-0.024407	2.485803
125.873150	1987.958779	5.517402	-0.024453	2.490405
125.964343	1996.063486	5.522406	-0.024475	2.495009
126.252133	2004.117808	5.527411	-0.024533	2.499590
126.495291	2012.150838	5.532416	-0.024584	2.504148
126.972187	2020.218394	5.537421	-0.024678	2.508734
127.517213	2028.296972	5.542426	-0.024784	2.513323
127.775535	2036.342719	5.547430	-0.024837	2.517864
128.057066	2044.385146	5.552435	-0.024895	2.522396
128.202393	2052.431214	5.557440	-0.024927	2.526913
128.696823	2060.489330	5.562445	-0.025024	2.531453
129.049492	2068.536655	5.567450	-0.025095	2.535969
129.248333	2076.589275	5.572454	-0.025137	2.540469
129.703508	2084.635191	5.577459	-0.025227	2.544975
130.002490	2092.676949	5.582464	-0.025288	2.549459
130.369575	2100.755998	5.587469	-0.025361	2.553962
130.699678	2108.805922	5.592474	-0.025428	2.558437
131.061392	2116.829085	5.597478	-0.025500	2.562892
131.113072	2124.931681	5.602483	-0.025515	2.567362
131.382596	2132.976664	5.607488	-0.025570	2.571807
131.697668	2141.058163	5.612493	-0.025634	2.576268
131.987916	2149.088035	5.617498	-0.025693	2.580690
132.467478	2157.101249	5.622502	-0.025788	2.585109
132.714157	2165.191118	5.627507	-0.025839	2.589547
132.835413	2173.434166	5.632512	-0.025866	2.594051
133.223528	2181.447971	5.637517	-0.025944	2.598441
133.803487	2189.403643	5.642522	-0.026057	2.602805
134.082045	2197.419777	5.647526	-0.026114	2.607175
134.402186	2205.486752	5.652531	-0.026178	2.611567
134.755772	2213.511651	5.657536	-0.026249	2.615931
135.187515	2221.538165	5.662541	-0.026335	2.620294
135.305825	2229.574807	5.667546	-0.026362	2.624634
135.500216	2237.645038	5.672550	-0.026403	2.628990
135.999124	2245.684806	5.677555	-0.026501	2.633342
136.148989	2253.740404	5.682560	-0.026534	2.637673
136.464638	2261.784572	5.687565	-0.026598	2.642001
136.647742	2269.819829	5.692570	-0.026637	2.646309
136.708377	2277.901166	5.697574	-0.026654	2.650626
137.186748	2285.955435	5.702579	-0.026748	2.654949
137.592808	2293.965592	5.707584	-0.026829	2.659237
138.129275	2302.000661	5.712589	-0.026934	2.663539
138.206852	2310.080793	5.717594	-0.026953	2.667829
138.578141	2318.148882	5.722598	-0.027027	2.672124
139.102831	2326.206822	5.727603	-0.027130	2.676417
139.323566	2334.231382	5.732608	-0.027176	2.680666
139.555529	2342.266858	5.737613	-0.027225	2.684914
139.777083	2350.308147	5.742618	-0.027271	2.689158
140.148605	2358.358459	5.747622	-0.027345	2.693410
140.494378	2366.407538	5.752627	-0.027415	2.697652
140.654376	2374.457224	5.757632	-0.027450	2.701877
141.066743	2382.488112	5.762637	-0.027531	2.706100
141.256434	2390.553696	5.767642	-0.027572	2.710322
141.622571	2398.604261	5.772646	-0.027645	2.714539
142.008671	2406.654973	5.777651	-0.027722	2.718752
142.145864	2414.674712	5.782656	-0.027753	2.722926
142.172039	2422.758619	5.787661	-0.027763	2.727121
142.622251	2430.781653	5.792666	-0.027852	2.731303
142.983529	2438.835662	5.797670	-0.027924	2.735490
143.444025	2446.877153	5.802675	-0.028015	2.739670
143.524273	2454.908904	5.807680	-0.028035	2.743815
143.889979	2462.966486	5.812685	-0.028108	2.747984
144.030231	2471.070402	5.817690	-0.028139	2.752157
144.337321	2479.138449	5.822694	-0.028202	2.756316
145.004333	2487.129000	5.827699	-0.028331	2.760450
145.429953	2495.100997	5.832704	-0.028415	2.764554
145.585552	2503.191335	5.837709	-0.028449	2.768696
145.798041	2511.259054	5.842714	-0.028494	2.772823
146.434864	2519.248283	5.847718	-0.028618	2.776930
146.439306	2527.347981	5.852723	-0.028624	2.781049
146.746200	2535.337137	5.857728	-0.028686	2.785124
147.093579	2543.387694	5.862733	-0.028756	2.789227
147.488730	2551.457109	5.867738	-0.028834	2.793335
147.725495	2559.464268	5.872742	-0.028883	2.797397
148.029764	2567.522440	5.877747	-0.028945	2.801482
148.137038	2575.557017	5.882752	-0.028970	2.805538
148.449609	2583.612541	5.887757	-0.029034	2.809611
148.619108	2591.672143	5.892762	-0.029070	2.813671
149.010283	2599.695010	5.897766	-0.029148	2.817720
149.413005	2607.745775	5.902771	-0.029228	2.821778
149.318138	2615.809093	5.907776	-0.029216	2.825808
149.840371	2623.835283	5.912781	-0.029318	2.829848
150.208615	2631.912712	5.917786	-0.029392	2.833900
150.509377	2639.917420	5.922790	-0.029453	2.837905
150.956448	2647.962197	5.927795	-0.029541	2.841933
151.246103	2655.970472	5.932800	-0.029600	2.845928
151.358447	2664.038578	5.937805	-0.029626	2.849938
151.789290	2672.094096	5.942810	-0.029711	2.853953
152.274573	2680.104543	5.947814	-0.029807	2.857943
152.570910	2688.161021	5.952819	-0.029867	2.861940
152.696148	2696.190544	5.957824	-0.029895	2.865908
152.976617	2704.241115	5.962829	-0.029953	2.869890
153.426863	2712.291624	5.967834	-0.030042	2.873876
153.615646	2720.321127	5.972838	-0.030082	2.877831
153.980933	2728.359907	5.977843	-0.030155	2.881795
154.185959	2736.378088	5.982848	-0.030198	2.885734
154.328369	2744.434107	5.987853	-0.030230	2.889684
154.658683	2752.495065	5.992858	-0.030297	2.893640
154.999444	2760.509100	5.997862	-0.030365	2.897569
155.459336	2768.558205	6.002867	-0.030456	2.901516
155.505593	2776.585899	6.007872	-0.030470	2.905425
155.805712	2784.647226	6.012877	-0.030531	2.909358
155.794599	2792.800892	6.017882	-0.030534	2.913314
155.858067	2800.832386	6.022886	-0.030551	2.917210
156.145110	2808.834638	6.027891	-0.030609	2.921098
156.419693	2816.811587	6.032896	-0.030665	2.924968
156.679319	2824.847489	6.037901	-0.030719	2.928861
156.791369	2832.906443	6.042906	-0.030745	2.932751
157.147978	2840.920973	6.047910	-0.030816	2.936628
157.552236	2848.948258	6.052915	-0.030896	2.940508
157.862392	2856.941276	6.057920	-0.030959	2.944362
158.043193	2865.016939	6.062925	-0.030998	2.948244
158.243199	2873.088224	6.067930	-0.031040	2.952119
158.322107	2881.132347	6.072934	-0.031060	2.955970
158.677507	2889.117969	6.077939	-0.031131	2.959802
159.047438	2897.147284	6.082944	-0.031205	2.963651
159.162950	2905.212590	6.087949	-0.031232	2.967499
159.340827	2913.262706	6.092954	-0.031270	2.971338
159.765183	2921.277897	6.097958	-0.031354	2.975168
159.928285	2929.331544	6.102963	-0.031390	2.978997
160.071526	2937.363486	6.107968	-0.031421	2.982811
160.360334	2945.392942	6.112973	-0.031480	2.986626
160.549805	2953.442712	6.117978	-0.031521	2.990440
160.646210	2961.514055	6.122982	-0.031544	2.994255
161.080250	2969.524245	6.127987	-0.031630	2.998054
161.316789	2977.513274	6.132992	-0.031679	3.001827
161.800355	2985.524309	6.137997	-0.031774	3.005618
162.015421	2993.577963	6.143002	-0.031819	3.009412
162.101468	3001.659443	6.148006	-0.031840	3.013207
162.523034	3009.693320	6.153011	-0.031924	3.016991
162.758002	3017.708297	6.158016	-0.031973	3.020753
162.980856	3025.733991	6.163021	-0.032019	3.024514
163.326708	3033.760324	6.168026	-0.032089	3.028277
163.553074	3041.826683	6.173030	-0.032136	3.032048
163.749442	3049.900956	6.178035	-0.032178	3.035817
163.940860	3057.888469	6.183040	-0.032218	3.039540
164.149341	3065.915059	6.188045	-0.032262	3.043278
164.287847	3073.963571	6.193050	-0.032293	3.047018
164.612493	3081.986005	6.198054	-0.032359	3.050750
165.065078	3090.053212	6.203059	-0.032448	3.054504
164.993363	3098.099924	6.208064	-0.032440	3.058219
165.126605	3106.129293	6.213069	-0.032470	3.061932
165.638271	3114.128416	6.218074	-0.032570	3.065643
165.942093	3122.138371	6.223078	-0.032632	3.069346
166.075896	3130.288247	6.228083	-0.032662	3.073100
166.422038	3138.314349	6.233088	-0.032731	3.076803
166.676653	3146.296269	6.238093	-0.032784	3.080476
166.733382	3154.314720	6.243098	-0.032799	3.084153
167.174562	3162.313453	6.248102	-0.032886	3.087834
167.392628	3170.382069	6.253107	-0.032932	3.091533
167.697238	3178.425063	6.258112	-0.032994	3.095219
167.740103	3186.445211	6.263117	-0.033007	3.098878
168.092862	3194.455430	6.268122	-0.033078	3.102543
168.406909	3202.489482	6.273126	-0.033141	3.106212
168.669810	3210.536938	6.278131	-0.033195	3.109881
168.886042	3218.579422	6.283136	-0.033241	3.113540
169.153959	3226.619448	6.288141	-0.033296	3.117197
169.280853	3234.669962	6.293146	-0.033324	3.120848
169.443224	3242.636664	6.298150	-0.033360	3.124458
169.850169	3250.712242	6.303155	-0.033441	3.128125
170.014260	3258.752956	6.308160	-0.033476	3.131760
170.378537	3266.784753	6.313165	-0.033549	3.135396
170.637938	3274.817646	6.318170	-0.033603	3.139023
170.949541	3282.801345	6.323174	-0.033666	3.142627
171.295311	3290.862666	6.328179	-0.033735	3.146262
171.289991	3298.914210	6.333184	-0.033739	3.149874
171.775287	3306.939658	6.338189	-0.033835	3.153491
171.757115	3315.025711	6.343194	-0.033836	3.157109
171.787638	3322.997513	6.348198	-0.033847	3.160674
172.190023	3331.021305	6.353203	-0.033927	3.164274
172.386338	3339.039381	6.358208	-0.033969	3.167859
172.571294	3347.102798	6.363213	-0.034008	3.171459
172.949409	3355.129473	6.368218	-0.034084	3.175047
173.015145	3363.164567	6.373222	-0.034101	3.178622
173.318088	3371.182443	6.378227	-0.034163	3.182195
173.417017	3379.187487	6.383232	-0.034186	3.185749
173.784186	3387.238624	6.388237	-0.034260	3.189331
174.155866	3395.299983	6.393242	-0.034334	3.192914
174.455174	3403.330840	6.398246	-0.034395	3.196476
174.981730	3411.315951	6.403251	-0.034498	3.200024
175.218406	3419.336986	6.408256	-0.034547	3.203571
175.565748	3427.413285	6.413261	-0.034617	3.207143
175.775177	3435.460687	6.418266	-0.034661	3.210693
176.069297	3443.480691	6.423270	-0.034721	3.214230
176.193601	3451.556255	6.428275	-0.034749	3.217781
176.289093	3459.551630	6.433280	-0.034772	3.221291
176.840694	3467.518030	6.438285	-0.034880	3.224804
177.087687	3475.578271	6.443290	-0.034931	3.228341
177.062070	3483.676493	6.448294	-0.034931	3.231880
177.370962	3491.753866	6.453299	-0.034994	3.235419
177.702685	3499.689154	6.458304	-0.035060	3.238894
177.849291	3507.702636	6.463309	-0.035093	3.242391
178.104099	3515.749287	6.468314	-0.035145	3.245903
178.527249	3523.734632	6.473318	-0.035229	3.249392
178.823856	3531.781432	6.478323	-0.035290	3.252898
178.851402	3539.833005	6.483328	-0.035300	3.256392
179.353160	3547.829548	6.488333	-0.035398	3.259877
179.826768	3555.837477	6.493338	-0.035491	3.263362
179.664981	3563.914427	6.498342	-0.035466	3.266848
179.936484	3571.970552	6.503347	-0.035522	3.270338
180.234673	3579.988110	6.508352	-0.035583	3.273809
180.581630	3588.024396	6.513357	-0.035652	3.277287
180.627219	3596.044457	6.518362	-0.035666	3.280742
180.640255	3604.035272	6.523366	-0.035673	3.284179
181.133823	3612.081279	6.528371	-0.035770	3.287655
181.186941	3620.128383	6.533376	-0.035785	3.291111
181.632357	3628.163318	6.538381	-0.035873	3.294573
181.915559	3636.184996	6.543386	-0.035931	3.298019
181.733139	3644.232750	6.548390	-0.035902	3.301455
182.108083	3652.225920	6.553395	-0.035977	3.304886
182.468551	3660.245699	6.558400	-0.036049	3.308323
182.791993	3668.316107	6.563405	-0.036115	3.311777
182.896077	3676.386687	6.568410	-0.036139	3.315220
183.164057	3684.363879	6.573414	-0.036194	3.318625
183.479835	3692.404691	6.578419	-0.036258	3.322055
183.465842	3700.404317	6.583424	-0.036261	3.325452
183.757733	3708.432364	6.588429	-0.036320	3.328869
184.131976	3716.476328	6.593434	-0.036395	3.332293
184.178632	3724.505762	6.598438	-0.036409	3.335694
184.657345	3732.499806	6.603443	-0.036503	3.339093
185.022466	3740.522471	6.608448	-0.036576	3.342496
185.091006	3748.545962	6.613453	-0.036594	3.345886
185.444128	3756.609997	6.618458	-0.036665	3.349299
185.843485	3764.622821	6.623462	-0.036744	3.352689
186.301268	3772.690870	6.628467	-0.036834	3.356100
186.411107	3780.688829	6.633472	-0.036860	3.359467
186.915566	3788.684770	6.638477	-0.036959	3.362843
187.411490	3796.701637	6.643482	-0.037056	3.366224
187.439053	3804.729594	6.648486	-0.037066	3.369589
187.742435	3812.846511	6.653491	-0.037128	3.372999
188.125837	3820.882086	6.658496	-0.037205	3.376373
188.341352	3828.878847	6.663501	-0.037250	3.379722
188.666972	3836.888537	6.668506	-0.037315	3.383077
188.828545	3844.937435	6.673510	-0.037351	3.386439
189.314974	3852.957268	6.678515	-0.037446	3.389797
189.811983	3861.023431	6.683520	-0.037544	3.393171
189.972427	3869.095316	6.688525	-0.037579	3.396533
190.282754	3877.046912	6.693530	-0.037642	3.399846
190.476421	3885.020681	6.698534	-0.037683	3.403161
190.700335	3893.069126	6.703539	-0.037730	3.406505
190.729383	3901.088246	6.708544	-0.037740	3.409827
191.023942	3909.136210	6.713549	-0.037800	3.413167
191.282194	3917.179337	6.718554	-0.037853	3.416500
191.525851	3925.140873	6.723558	-0.037904	3.419796
191.958915	3933.179413	6.728563	-0.037989	3.423126
192.057747	3941.234515	6.733568	-0.038013	3.426449
192.430686	3949.235560	6.738573	-0.038087	3.429755
192.712712	3957.305106	6.743578	-0.038145	3.433084
193.036561	3965.326757	6.748582	-0.038210	3.436391
193.202990	3973.335628	6.753587	-0.038246	3.439684
193.311781	3981.359986	6.758592	-0.038272	3.442978
193.498928	3989.388788	6.763597	-0.038312	3.446274
193.746947	3997.425027	6.768602	-0.038363	3.449571
193.862474	4005.448445	6.773606	-0.038390	3.452856
194.080905	4013.543921	6.778611	-0.038435	3.456170
194.246894	4021.517553	6.783616	-0.038471	3.459430
194.468217	4029.546451	6.788621	-0.038518	3.462711
194.967555	4037.553205	6.793626	-0.038616	3.465988
195.145310	4045.571137	6.798630	-0.038654	3.469257
195.558072	4053.642578	6.803635	-0.038736	3.472552
195.746528	4061.690451	6.808640	-0.038776	3.475827
195.933849	4069.666048	6.813645	-0.038816	3.479070
196.168770	4077.709370	6.818650	-0.038865	3.482338
196.205508	4085.687276	6.823654	-0.038877	3.485571
196.697376	4093.706355	6.828659	-0.038973	3.488831
197.183211	4101.735190	6.833664	-0.039069	3.492092
197.355885	4109.759872	6.838669	-0.039106	3.495339
197.576802	4117.818532	6.843674	-0.039152	3.498598
197.738316	4125.832097	6.848678	-0.039187	3.501833
198.049744	4133.832228	6.853683	-0.039251	3.505065
198.357150	4141.873582	6.858688	-0.039313	3.508311
198.559815	4149.933716	6.863693	-0.039356	3.511557
198.748600	4157.973704	6.868698	-0.039396	3.514792
198.777992	4165.984385	6.873702	-0.039406	3.518007
199.205028	4174.004702	6.878707	-0.039491	3.521236
199.471674	4181.951249	6.883712	-0.039546	3.524427
199.626086	4190.040119	6.888717	-0.039580	3.527669
199.909811	4198.092310	6.893722	-0.039638	3.530896
200.088701	4206.122414	6.898726	-0.039676	3.534109
200.519184	4214.153427	6.903731	-0.039761	3.537327
200.515746	4222.180005	6.908736	-0.039766	3.540527
200.952669	4230.171338	6.913741	-0.039852	3.543723
201.128009	4238.220314	6.918746	-0.039890	3.546932
201.177475	4246.225591	6.923750	-0.039904	3.550116
201.426642	4254.371792	6.928755	-0.039956	3.553360
201.589076	4262.432851	6.933760	-0.039991	3.556564
201.702441	4270.344213	6.938765	-0.040017	3.559704
202.043766	4278.320645	6.943770	-0.040086	3.562874
202.216189	4286.316021	6.948774	-0.040123	3.566044
202.403167	4294.359382	6.953779	-0.040163	3.569231
202.512026	4302.405482	6.958784	-0.040188	3.572413
202.953157	4310.425779	6.963789	-0.040275	3.575592
203.301166	4318.430921	6.968794	-0.040345	3.578759
203.374107	4326.454633	6.973798	-0.040364	3.581923
203.822592	4334.447094	6.978803	-0.040452	3.585082
204.069378	4342.476514	6.983808	-0.040503	3.588248
204.446582	4350.538690	6.988813	-0.040579	3.591427
204.656106	4358.574133	6.993818	-0.040623	3.594588
204.971147	4366.574933	6.998822	-0.040687	3.597735
205.239862	4374.607725	7.003827	-0.040742	3.600891
205.436176	4382.596239	7.008832	-0.040783	3.604025
205.663281	4390.642292	7.013837	-0.040831	3.607180
206.085133	4398.639311	7.018842	-0.040914	3.610318
206.094121	4406.682344	7.023846	-0.040921	3.613459
206.357206	4414.770454	7.028851	-0.040975	3.616623
206.526657	4422.739392	7.033856	-0.041012	3.619735
206.780923	4430.779864	7.038861	-0.041064	3.622874
206.983897	4438.785286	7.043866	-0.041107	3.625995
207.149218	4446.796320	7.048870	-0.041143	3.629115
207.492878	4454.876655	7.053875	-0.041212	3.632264
207.894976	4462.888496	7.058880	-0.041292	3.635385
208.227647	4470.900949	7.063885	-0.041359	3.638502
208.719401	4478.930386	7.068890	-0.041456	3.641626
208.598661	4486.922855	7.073894	-0.041438	3.644718
209.141998	4494.956343	7.078899	-0.041545	3.647840
209.433857	4502.997232	7.083904	-0.041604	3.650956
209.544309	4511.037308	7.088909	-0.041630	3.654064
209.786552	4519.062353	7.093914	-0.041680	3.657167
210.165781	4527.043704	7.098918	-0.041755	3.660254
210.403913	4535.075583	7.103923	-0.041805	3.663354
210.653444	4543.099002	7.108928	-0.041856	3.666448
210.811782	4551.121654	7.113933	-0.041891	3.669538
211.047128	4559.234575	7.118938	-0.041940	3.672661
211.093686	4567.217461	7.123942	-0.041954	3.675727
211.669575	4575.213216	7.128947	-0.042066	3.678808
211.863877	4583.241348	7.133952	-0.042107	3.681890
212.093083	4591.211178	7.138957	-0.042155	3.684948
212.269006	4599.276976	7.143962	-0.042193	3.688038
212.466626	4607.311428	7.148966	-0.042235	3.691115
212.616915	4615.384412	7.153971	-0.042268	3.694202
212.889047	4623.346565	7.158976	-0.042324	3.697248
212.914087	4631.335670	7.163981	-0.042333	3.700295
213.369993	4639.386069	7.168986	-0.042423	3.703373
213.573800	4647.400699	7.173990	-0.042466	3.706429
214.015131	4655.423885	7.178995	-0.042553	3.709492
214.189539	4663.503207	7.184000	-0.042591	3.712567
214.384642	4671.568239	7.189005	-0.042633	3.715634
214.534010	4679.545011	7.194010	-0.042665	3.718665
214.855441	4687.516516	7.199014	-0.042730	3.721694
215.272760	4695.502560	7.204019	-0.042813	3.724730
215.264561	4703.549629	7.209024	-0.042817	3.727775
215.586996	4711.574865	7.214029	-0.042882	3.730818
215.826842	4719.626078	7.219034	-0.042931	3.733866
215.805655	4727.637579	7.224038	-0.042933	3.736890
216.270811	4735.634919	7.229043	-0.043024	3.739918
216.487441	4743.661161	7.234048	-0.043070	3.742949
216.729381	4751.671696	7.239053	-0.043120	3.745971
216.935271	4759.730898	7.244058	-0.043163	3.749009
217.207675	4767.757717	7.249062	-0.043219	3.752034
217.419912	4775.796528	7.254067	-0.043264	3.755059
217.463360	4783.803252	7.259072	-0.043277	3.758066
217.777738	4791.813902	7.264077	-0.043340	3.761078
218.190074	4799.805112	7.269082	-0.043422	3.764083
218.228270	4807.856621	7.274086	-0.043434	3.767099
218.582418	4815.900364	7.279091	-0.043506	3.770117
218.807062	4823.931014	7.284096	-0.043552	3.773124
219.133708	4831.969527	7.289101	-0.043618	3.776135
219.245480	4839.965658	7.294106	-0.043644	3.779122
219.508038	4848.013528	7.299110	-0.043698	3.782130
220.080416	4855.975607	7.304115	-0.043810	3.785110
220.377887	4864.007612	7.309120	-0.043870	3.788108
220.661924	4872.052792	7.314125	-0.043928	3.791108
220.919889	4880.106864	7.319130	-0.043981	3.794108
221.085126	4888.134246	7.324134	-0.044017	3.797094
221.395090	4896.107326	7.329139	-0.044080	3.800061
221.726206	4904.107427	7.334144	-0.044147	3.803035
222.074318	4912.101991	7.339149	-0.044217	3.806006
222.626640	4920.143324	7.344154	-0.044325	3.808996
222.521223	4928.178015	7.349158	-0.044310	3.811967
223.058730	4936.207830	7.354163	-0.044415	3.814947
223.176757	4944.243054	7.359168	-0.044442	3.817919
223.501338	4952.254084	7.364173	-0.044508	3.820883
223.915445	4960.270576	7.369178	-0.044590	3.823849
223.897153	4968.286022	7.374182	-0.044592	3.826803
224.090441	4976.300682	7.379187	-0.044633	3.829759
224.328477	4984.367455	7.384192	-0.044682	3.832733
224.598743	4992.372532	7.389197	-0.044737	3.835682
224.968620	5000.398671	7.394202	-0.044811	3.838639
224.967855	5008.413734	7.399206	-0.044816	3.841582
225.339398	5016.368112	7.404211	-0.044891	3.844507
225.380853	5024.439163	7.409216	-0.044903	3.847467
225.661550	5032.428109	7.414221	-0.044961	3.850399
226.100465	5040.512622	7.419226	-0.045048	3.853367
226.014075	5048.515611	7.424230	-0.045037	3.856293
226.154991	5056.553147	7.429235	-0.045068	3.859233
226.348156	5064.588027	7.434240	-0.045109	3.862171
226.624095	5072.544136	7.439245	-0.045165	3.865080
227.027220	5080.591939	7.444250	-0.045246	3.868022
226.926749	5088.643391	7.449254	-0.045232	3.870954
227.552490	5096.868368	7.454259	-0.045354	3.873961
227.632260	5104.913094	7.459264	-0.045374	3.876889
227.560454	5112.776195	7.464269	-0.045365	3.879746
227.936166	5120.759546	7.469274	-0.045440	3.882653
228.042464	5128.710066	7.474278	-0.045465	3.885541
228.464408	5136.733309	7.479283	-0.045549	3.888459
228.685111	5144.782037	7.484288	-0.045595	3.891380
228.972355	5152.779075	7.489293	-0.045653	3.894282
229.155368	5160.862769	7.494298	-0.045693	3.897211
229.130393	5168.833961	7.499302	-0.045693	3.900093
229.490804	5176.832435	7.504307	-0.045765	3.902989
229.709441	5184.865139	7.509312	-0.045811	3.905894
230.025503	5192.862522	7.514317	-0.045875	3.908785
230.266506	5200.934811	7.519322	-0.045925	3.911700
230.299106	5208.968453	7.524326	-0.045936	3.914595
230.440194	5216.986893	7.529331	-0.045967	3.917484
230.824564	5224.958979	7.534336	-0.046044	3.920358
231.002510	5232.963210	7.539341	-0.046082	3.923239
231.016871	5241.020810	7.544346	-0.046090	3.926133
231.124723	5249.021357	7.549350	-0.046115	3.929007
231.666667	5257.048690	7.554355	-0.046221	3.931895
231.978184	5265.071903	7.559360	-0.046284	3.934776
231.990590	5273.074174	7.564365	-0.046292	3.937642
232.451757	5281.066130	7.569370	-0.046382	3.940511
232.730933	5289.070486	7.574374	-0.046440	3.943378
233.030945	5297.117351	7.579379	-0.046500	3.946259
233.239367	5305.149356	7.584384	-0.046544	3.949130
233.263571	5313.201550	7.589389	-0.046554	3.952004
233.589510	5321.236187	7.594394	-0.046620	3.954874
233.628661	5329.246871	7.599398	-0.046632	3.957729
233.865351	5337.226637	7.604403	-0.046681	3.960574
233.885934	5345.242824	7.609408	-0.046690	3.963426
234.222235	5353.243540	7.614413	-0.046758	3.966276
234.587111	5361.298909	7.619418	-0.046831	3.969144
234.866542	5369.305378	7.624422	-0.046888	3.971991
235.138806	5377.368239	7.629427	-0.046944	3.974856
235.448068	5385.347192	7.634432	-0.047006	3.977689
235.794565	5393.369021	7.639437	-0.047076	3.980537
236.115625	5401.382935	7.644442	-0.047141	3.983379
236.114690	5409.401792	7.649446	-0.047146	3.986215
236.422184	5417.466870	7.654451	-0.047208	3.989071
236.775179	5425.480945	7.659456	-0.047279	3.991907
236.937672	5433.529089	7.664461	-0.047314	3.994750
237.218910	5441.558133	7.669466	-0.047372	3.997586
237.422312	5449.527429	7.674470	-0.047415	4.000398
237.779573	5457.572600	7.679475	-0.047486	4.003238
238.034120	5465.555509	7.684480	-0.047539	4.006051
238.299206	5473.580968	7.689485	-0.047593	4.008878
238.627769	5481.621811	7.694490	-0.047659	4.011709
238.631189	5489.646500	7.699494	-0.047665	4.014527
239.099486	5497.682030	7.704499	-0.047757	4.017354
239.474746	5505.659850	7.709504	-0.047832	4.020158
239.718397	5513.686618	7.714509	-0.047883	4.022975
240.025990	5521.723458	7.719514	-0.047945	4.025794
240.197977	5529.708611	7.724518	-0.047982	4.028591
240.720453	5537.781538	7.729523	-0.048085	4.031422
240.951898	5545.889913	7.734528	-0.048133	4.034259
241.036775	5553.875352	7.739533	-0.048154	4.037049
241.629745	5561.815088	7.744538	-0.048269	4.039828
241.758188	5569.800926	7.749542	-0.048298	4.042615
241.921811	5577.810561	7.754547	-0.048334	4.045408
242.110197	5585.856151	7.759552	-0.048374	4.048213
242.221854	5593.877424	7.764557	-0.048400	4.051006
242.412482	5601.903679	7.769562	-0.048440	4.053800
242.631271	5609.915513	7.774566	-0.048486	4.056587
242.875662	5617.925600	7.779571	-0.048537	4.059372
243.040974	5625.939157	7.784576	-0.048573	4.062155
243.399052	5633.878331	7.789581	-0.048644	4.064914
243.861393	5642.006247	7.794586	-0.048735	4.067737
243.747097	5650.025461	7.799590	-0.048719	4.070512
243.715389	5658.086476	7.804595	-0.048718	4.073302
243.910835	5666.083363	7.809600	-0.048760	4.076070
244.205255	5674.043855	7.814605	-0.048820	4.078825
244.610650	5682.086824	7.819610	-0.048900	4.081608
244.687153	5690.024528	7.824614	-0.048920	4.084349
244.995264	5698.107874	7.829619	-0.048982	4.087141
245.043003	5706.120117	7.834624	-0.048996	4.089903
245.169739	5714.151945	7.839629	-0.049025	4.092671
245.635428	5722.214202	7.844634	-0.049117	4.095452
245.698620	5730.175129	7.849638	-0.049133	4.098191
245.976363	5738.192216	7.854643	-0.049190	4.100950
246.054787	5746.232461	7.859648	-0.049210	4.103713
246.351055	5754.226190	7.864653	-0.049270	4.106460
246.527244	5762.298240	7.869658	-0.049308	4.109231
246.772110	5770.314919	7.874662	-0.049359	4.111983
247.010095	5778.343716	7.879667	-0.049408	4.114736
247.242813	5786.395528	7.884672	-0.049456	4.117495
247.384276	5794.336636	7.889677	-0.049488	4.120213
247.822492	5802.396337	7.894682	-0.049575	4.122974
247.909231	5810.388609	7.899686	-0.049596	4.125706
248.103691	5818.442660	7.904691	-0.049637	4.128458
248.427335	5826.437061	7.909696	-0.049702	4.131189
248.523699	5834.486330	7.914701	-0.049725	4.133935
248.938783	5842.523122	7.919706	-0.049808	4.136678
249.123759	5850.487436	7.924710	-0.049847	4.139392
249.449994	5858.572274	7.929715	-0.049913	4.142147
249.606835	5866.513407	7.934720	-0.049947	4.144849
249.723589	5874.545758	7.939725	-0.049974	4.147580
250.061317	5882.572969	7.944730	-0.050042	4.150310
250.098525	5890.637232	7.949734	-0.050054	4.153047
250.172098	5898.641117	7.954739	-0.050073	4.155762
250.359986	5906.634362	7.959744	-0.050113	4.158473
250.761097	5914.651435	7.964749	-0.050193	4.161193
251.016911	5922.668716	7.969754	-0.050245	4.163909
251.149902	5930.650254	7.974758	-0.050275	4.166610
251.526340	5938.680591	7.979763	-0.050350	4.169329
251.699533	5946.755482	7.984768	-0.050388	4.172059
251.752586	5954.738890	7.989773	-0.050403	4.174754
251.888716	5962.856200	7.994778	-0.050433	4.177494
252.068563	5970.744024	7.999782	-0.050472	4.180155
252.486900	5978.734842	8.004787	-0.050555	4.182852
252.502986	5986.778366	8.009792	-0.050563	4.185560
252.611784	5994.830622	8.014797	-0.050588	4.188271
252.809461	6002.863935	8.019802	-0.050630	4.190974
252.870018	6010.941278	8.024806	-0.050646	4.193689
253.277336	6018.944090	8.029811	-0.050727	4.196381
253.556362	6026.886457	8.034816	-0.050784	4.199049
253.714731	6034.885261	8.039821	-0.050819	4.201734
254.313599	6042.883947	8.044826	-0.050935	4.204421
254.434110	6050.942869	8.049830	-0.050963	4.207121
254.556879	6058.925787	8.054835	-0.050991	4.209795
254.873718	6067.000343	8.059840	-0.051055	4.212499
255.392736	6074.990957	8.064845	-0.051157	4.215175
255.593293	6083.031977	8.069850	-0.051199	4.217864
255.612816	6090.991961	8.074854	-0.051208	4.220522
255.999581	6099.020945	8.079859	-0.051285	4.223204
256.455947	6107.022239	8.084864	-0.051375	4.225877
256.391792	6115.034680	8.089869	-0.051368	4.228546
256.672466	6123.119959	8.094874	-0.051425	4.231241
257.004267	6131.118950	8.099878	-0.051492	4.233906
257.129013	6139.180719	8.104883	-0.051521	4.236589
257.247227	6147.147305	8.109888	-0.051548	4.239238
257.518192	6155.155026	8.114893	-0.051603	4.241900
257.801374	6163.129921	8.119898	-0.051661	4.244550
257.858427	6171.183081	8.124902	-0.051677	4.247222
258.074150	6179.172884	8.129907	-0.051722	4.249873
258.274344	6187.265283	8.134912	-0.051764	4.252556
258.485131	6195.265446	8.139917	-0.051809	4.255207
258.795049	6203.311410	8.144922	-0.051871	4.257873
259.060479	6211.283478	8.149926	-0.051926	4.260511
259.359158	6219.322079	8.154931	-0.051987	4.263171
259.503438	6227.364260	8.159936	-0.052019	4.265828
259.561834	6235.392974	8.164941	-0.052035	4.268479
259.805127	6243.424705	8.169946	-0.052085	4.271130
259.964607	6251.442871	8.174950	-0.052120	4.273775
260.255738	6259.459835	8.179955	-0.052179	4.276418
260.477787	6267.453302	8.184960	-0.052225	4.279052
260.663780	6275.464096	8.189965	-0.052265	4.281690
260.937126	6283.487205	8.194970	-0.052321	4.284330
261.089713	6291.468990	8.199974	-0.052355	4.286955
261.340674	6299.510344	8.204979	-0.052406	4.289598
261.560974	6307.547056	8.209984	-0.052452	4.292237
261.766442	6315.562517	8.214989	-0.052496	4.294868
262.099744	6323.641805	8.219994	-0.052563	4.297519
262.022427	6331.552127	8.224998	-0.052554	4.300110
262.297885	6339.600896	8.230003	-0.052610	4.302748
262.713113	6347.574109	8.235008	-0.052692	4.305360
262.711653	6355.630877	8.240013	-0.052697	4.307995
262.772386	6363.672980	8.245018	-0.052714	4.310623
263.103011	6371.686066	8.250022	-0.052780	4.313243
263.303936	6379.719571	8.255027	-0.052823	4.315867
263.407984	6387.706640	8.260032	-0.052847	4.318473
263.493650	6395.691332	8.265037	-0.052868	4.321077
263.785544	6403.714623	8.270042	-0.052928	4.323693
263.927812	6411.732779	8.275046	-0.052959	4.326305
264.086110	6419.759333	8.280051	-0.052994	4.328918
264.501533	6427.789065	8.285056	-0.053076	4.331532
264.546486	6435.796244	8.290061	-0.053090	4.334135
264.959916	6443.841746	8.295066	-0.053172	4.336752
264.848285	6451.825451	8.300070	-0.053156	4.339342
265.093620	6459.865134	8.305075	-0.053207	4.341952
265.391728	6467.842208	8.310080	-0.053267	4.344541
265.549358	6475.850182	8.315085	-0.053302	4.347137
265.763347	6483.885974	8.320090	-0.053347	4.349741
265.797309	6491.949602	8.325094	-0.053358	4.352351
266.059833	6500.048287	8.330099	-0.053412	4.354972
266.306130	6508.022830	8.335104	-0.053463	4.357551
266.511841	6515.931465	8.340109	-0.053506	4.360108
266.863460	6524.009335	8.345114	-0.053577	4.362718
266.990976	6531.975512	8.350118	-0.053606	4.365289
267.092371	6539.972118	8.355123	-0.053630	4.367869
267.296343	6547.995796	8.360128	-0.053673	4.370456
267.472621	6556.072340	8.365133	-0.053711	4.373058
267.783214	6564.090184	8.370138	-0.053773	4.375641
267.967025	6572.065698	8.375142	-0.053813	4.378208
267.935032	6580.073171	8.380147	-0.053812	4.380782
268.134397	6588.118157	8.385152	-0.053854	4.383369
268.289314	6596.085136	8.390157	-0.053888	4.385928
268.709856	6604.127130	8.395162	-0.053971	4.388511
268.806433	6612.145545	8.400166	-0.053994	4.391084
269.246841	6620.185258	8.405171	-0.054081	4.393664
269.626819	6628.266963	8.410176	-0.054157	4.396255
269.770838	6636.196592	8.415181	-0.054189	4.398795
270.167861	6644.243816	8.420186	-0.054268	4.401372
270.140330	6652.204198	8.425190	-0.054268	4.403918
270.330149	6660.259488	8.430195	-0.054309	4.406493
270.531770	6668.273438	8.435200	-0.054351	4.409054
270.681965	6676.272400	8.440205	-0.054384	4.411609
270.798578	6684.337268	8.445210	-0.054411	4.414182
271.017050	6692.357352	8.450214	-0.054457	4.416741
271.524154	6700.398408	8.455219	-0.054556	4.419306
271.466223	6708.466482	8.460224	-0.054551	4.421875
271.496682	6716.400585	8.465229	-0.054561	4.424401
271.895395	6724.466424	8.470234	-0.054641	4.426969
272.084284	6732.428140	8.475238	-0.054681	4.429501
272.213562	6740.474940	8.480243	-0.054710	4.432059
272.276761	6748.546050	8.485248	-0.054727	4.434622
272.529246	6756.518907	8.490253	-0.054779	4.437154
272.656666	6764.512882	8.495258	-0.054808	4.439690
273.101272	6772.550602	8.500262	-0.054896	4.442240
273.307199	6780.494739	8.505267	-0.054939	4.444758
273.042928	6788.570854	8.510272	-0.054895	4.447314
273.276592	6796.531696	8.515277	-0.054943	4.449835
273.641369	6804.622871	8.520282	-0.055017	4.452395
273.803258	6812.626524	8.525286	-0.055052	4.454926
273.834442	6820.645284	8.530291	-0.055063	4.457460
274.232526	6828.621709	8.535296	-0.055142	4.459980
274.262512	6836.668497	8.540301	-0.055152	4.462519
274.549596	6844.651562	8.545306	-0.055211	4.465038
274.609322	6852.689397	8.550310	-0.055227	4.467572
274.927740	6860.687299	8.555315	-0.055292	4.470093
274.814107	6868.778904	8.560320	-0.055276	4.472640
275.060347	6876.747147	8.565325	-0.055326	4.475148
275.534890	6884.757265	8.570330	-0.055420	4.477669
275.750995	6892.705230	8.575335	-0.055465	4.480168
275.745989	6900.764365	8.580339	-0.055469	4.482699
276.159089	6908.754247	8.585344	-0.055551	4.485209
276.345431	6916.769911	8.590349	-0.055591	4.487725
276.527054	6924.853931	8.595354	-0.055630	4.490260
276.609002	6932.852869	8.600359	-0.055650	4.492768
276.878501	6940.882498	8.605363	-0.055706	4.495284
276.939571	6948.865754	8.610368	-0.055722	4.497783
276.938990	6956.866005	8.615373	-0.055727	4.500286
277.332370	6964.906257	8.620378	-0.055805	4.502802
277.536402	6972.867836	8.625383	-0.055848	4.505291
277.757125	6980.940741	8.630387	-0.055894	4.507813
277.940936	6988.953540	8.635392	-0.055934	4.510315
277.921368	6996.996488	8.640397	-0.055935	4.512824
278.249528	7005.070287	8.645402	-0.056001	4.515343
278.259769	7013.039886	8.650407	-0.056008	4.517827
278.507747	7020.998114	8.655411	-0.056060	4.520306
279.006632	7029.022234	8.660416	-0.056158	4.522805
279.041765	7036.960852	8.665421	-0.056169	4.525276
279.282881	7045.053081	8.670426	-0.056219	4.527792
279.549647	7053.070371	8.675431	-0.056274	4.530285
279.765605	7061.082456	8.680435	-0.056319	4.532774
280.068851	7069.118621	8.685440	-0.056381	4.535269
280.140429	7077.086231	8.690445	-0.056399	4.537742
280.401925	7085.104465	8.695450	-0.056453	4.540229
280.485369	7093.110053	8.700455	-0.056474	4.542710
280.644427	7101.121671	8.705459	-0.056508	4.545192
280.908315	7109.182590	8.710464	-0.056562	4.547688
281.181690	7117.145060	8.715469	-0.056618	4.550152
281.385954	7125.242553	8.720474	-0.056662	4.552657
281.628052	7133.241363	8.725479	-0.056712	4.555129
281.892418	7141.293049	8.730483	-0.056766	4.557617
281.919283	7149.273361	8.735488	-0.056776	4.560081
282.301021	7157.271780	8.740493	-0.056852	4.562549
282.446405	7165.260390	8.745498	-0.056884	4.565013
282.535881	7173.294105	8.750503	-0.056906	4.567490
282.690660	7181.285372	8.755507	-0.056940	4.569952
282.971920	7189.360738	8.760512	-0.056997	4.572438
282.875272	7197.367669	8.765517	-0.056985	4.574902
283.087824	7205.462295	8.770522	-0.057029	4.577392
283.340704	7213.389626	8.775527	-0.057081	4.579829
283.717129	7221.461259	8.780531	-0.057157	4.582309
283.669113	7229.406146	8.785536	-0.057153	4.584749
283.834957	7237.469806	8.790541	-0.057189	4.587224
284.053400	7245.475693	8.795546	-0.057234	4.589679
284.179316	7253.479998	8.800551	-0.057263	4.592133
284.420943	7261.553706	8.805555	-0.057313	4.594607
284.758100	7269.609314	8.810560	-0.057381	4.597074
285.004046	7277.504192	8.815565	-0.057432	4.599491
285.184289	7285.593261	8.820570	-0.057470	4.601965
285.414175	7293.511045	8.825575	-0.057518	4.604386
285.451943	7301.587495	8.830579	-0.057530	4.606854
285.655292	7309.572140	8.835584	-0.057573	4.609292
285.731240	7317.601007	8.840589	-0.057592	4.611743
286.081953	7325.660832	8.845594	-0.057663	4.614202
285.944834	7333.673734	8.850599	-0.057642	4.616645
286.099845	7341.621307	8.855603	-0.057676	4.619067
286.372846	7349.720838	8.860608	-0.057732	4.621534
286.339202	7357.593729	8.865613	-0.057731	4.623931
286.597588	7365.699892	8.870618	-0.057784	4.626398
286.682526	7373.690118	8.875623	-0.057805	4.628827
286.780231	7381.738029	8.880627	-0.057828	4.631273
286.982089	7389.789388	8.885632	-0.057871	4.633719
287.076287	7397.768773	8.890637	-0.057894	4.636142
287.545625	7405.784028	8.895642	-0.057986	4.638574
287.771762	7413.777385	8.900647	-0.058033	4.640998
288.029116	7421.751401	8.905651	-0.058086	4.643415
288.102976	7429.822984	8.910656	-0.058105	4.645861
288.096322	7437.836750	8.915661	-0.058109	4.648287
288.273363	7445.897574	8.920666	-0.058147	4.650727
288.587161	7453.875403	8.925671	-0.058210	4.653140
288.740577	7461.874508	8.930675	-0.058244	4.655558
289.147631	7469.937667	8.935680	-0.058325	4.657994
289.260299	7477.857261	8.940685	-0.058351	4.660386
289.471753	7485.973790	8.945690	-0.058395	4.662836
289.622577	7493.867744	8.950695	-0.058429	4.665217
289.730733	7501.998616	8.955699	-0.058454	4.667669
290.016557	7509.982320	8.960704	-0.058512	4.670075
290.106668	7518.006639	8.965709	-0.058534	4.672492
290.445266	7526.137009	8.970714	-0.058602	4.674939
290.598851	7534.095434	8.975719	-0.058636	4.677334
290.648930	7542.030448	8.980723	-0.058650	4.679720
291.067485	7550.078601	8.985728	-0.058733	4.682139
291.046414	7557.974711	8.990733	-0.058734	4.684511
291.404341	7566.076754	8.995738	-0.058806	4.686944
291.563048	7574.061228	9.000743	-0.058841	4.689340
291.656855	7582.152500	9.005747	-0.058863	4.691767
291.893352	7590.149996	9.010752	-0.058912	4.694164
292.005582	7598.104987	9.015757	-0.058938	4.696548
292.200001	7606.178288	9.020762	-0.058980	4.698966
292.297458	7614.169596	9.025767	-0.059003	4.701358
292.394895	7622.136840	9.030771	-0.059026	4.703741
292.631154	7630.187533	9.035776	-0.059075	4.706148
292.947690	7638.206501	9.040781	-0.059139	4.708545
293.322630	7646.253145	9.045786	-0.059214	4.710948
293.374091	7654.272136	9.050791	-0.059229	4.713342
293.457360	7662.230621	9.055795	-0.059249	4.715717
293.745062	7670.283886	9.060800	-0.059308	4.718118
293.865194	7678.279161	9.065805	-0.059335	4.720502
294.055465	7686.339938	9.070810	-0.059376	4.722903
294.119943	7694.292610	9.075815	-0.059393	4.725271
294.306784	7702.375279	9.080819	-0.059433	4.727677
294.538634	7710.368108	9.085824	-0.059481	4.730054
294.708151	7718.378103	9.090829	-0.059518	4.732436
294.847159	7726.459146	9.095834	-0.059549	4.734837
295.198806	7734.431916	9.100839	-0.059619	4.737205
295.247170	7742.422528	9.105843	-0.059633	4.739577
295.534297	7750.468073	9.110848	-0.059692	4.741964
295.575640	7758.421470	9.115853	-0.059705	4.744323
295.860708	7766.508948	9.120858	-0.059763	4.746719
295.858273	7774.477312	9.125863	-0.059767	4.749081
296.006960	7782.525156	9.130867	-0.059800	4.751464
296.328466	7790.621279	9.135872	-0.059865	4.753859
296.512161	7798.599691	9.140877	-0.059904	4.756219
296.714825	7806.510559	9.145882	-0.059947	4.758558
296.784935	7814.515727	9.150887	-0.059965	4.760924
296.955551	7822.526140	9.155891	-0.060002	4.763290
297.034543	7830.606098	9.160896	-0.060022	4.765675
297.345942	7838.610541	9.165901	-0.060085	4.768036
297.675232	7846.720938	9.170906	-0.060151	4.770427
297.609644	7854.716012	9.175911	-0.060144	4.772785
297.749595	7862.692301	9.180915	-0.060175	4.775135
297.746400	7870.690808	9.185920	-0.060180	4.777491
297.790380	7878.586773	9.190925	-0.060193	4.779815
298.154955	7886.653399	9.195930	-0.060266	4.782187
298.348488	7894.687809	9.200935	-0.060307	4.784549
298.537848	7902.694342	9.205939	-0.060347	4.786902
298.576634	7910.749497	9.210944	-0.060360	4.789268
298.581206	7918.707138	9.215949	-0.060366	4.791605
298.939111	7926.800493	9.220954	-0.060437	4.793979
299.058278	7934.816730	9.225959	-0.060465	4.796330
299.400434	7942.783887	9.230963	-0.060533	4.798665
299.618493	7950.817088	9.235968	-0.060579	4.801018
299.457659	7958.771682	9.240973	-0.060554	4.803349
299.841375	7966.803710	9.245978	-0.060631	4.805699
300.041331	7974.844368	9.250983	-0.060673	4.808051
300.020160	7982.828898	9.255987	-0.060674	4.810387
300.422921	7990.292298	9.260992	-0.060754	4.812567
300.448255	7994.750529	9.265997	-0.060761	4.813870
300.589243	7997.310789	9.271002	-0.060789	4.814617
300.841833	7998.576975	9.276007	-0.060837	4.814986
300.836333	7999.029989	9.281011	-0.060836	4.815118
301.163680	8000.052813	9.286016	-0.060897	4.815415
301.291930	8000.002552	9.291021	-0.060921	4.815400
301.519776	8000.022340	9.296026	-0.060963	4.815405
301.683110	7999.970521	9.301031	-0.060994	4.815389
301.826347	7999.971809	9.306035	-0.061020	4.815389
301.816188	8000.012241	9.311040	-0.061018	4.815400
301.831237	7999.946213	9.316045	-0.061021	4.815381
301.933181	8000.016288	9.321050	-0.061040	4.815401
301.874711	7999.937287	9.326055	-0.061029	4.815378
301.954331	7999.993098	9.331059	-0.061043	4.815394
302.309142	8000.040639	9.336064	-0.061109	4.815406
302.210224	7999.990893	9.341069	-0.061091	4.815392
302.281963	8000.015581	9.346074	-0.061104	4.815399
302.488705	7999.956999	9.351079	-0.061142	4.815381
302.413794	7999.926889	9.356083	-0.061128	4.815373
302.257962	7999.947810	9.361088	-0.061099	4.815380
302.352062	7999.931185	9.366093	-0.061116	4.815374
302.532199	7999.906364	9.371098	-0.061150	4.815366
302.414577	7999.931124	9.376103	-0.061128	4.815374
302.663133	7999.924536	9.381107	-0.061174	4.815371
302.817811	7999.920670	9.386112	-0.061202	4.815369
302.384116	7999.889966	9.391117	-0.061121	4.815362
302.527987	7999.987456	9.396122	-0.061148	4.815390
302.919125	8000.045219	9.401127	-0.061221	4.815405
302.870665	8000.025165	9.406131	-0.061212	4.815399
302.854540	8000.070843	9.411136	-0.061209	4.815413
302.989612	8000.010007	9.416141	-0.061233	4.815394
302.996398	7999.991936	9.421146	-0.061235	4.815389
302.738110	8000.033606	9.426151	-0.061186	4.815402
302.789217	7999.957485	9.431155	-0.061196	4.815380
303.099276	8000.021388	9.436160	-0.061253	4.815397
303.085808	7999.981606	9.441165	-0.061251	4.815385
303.380384	7999.977919	9.446170	-0.061305	4.815383
303.249124	8000.006728	9.451175	-0.061281	4.815392
303.153765	7999.980554	9.456179	-0.061263	4.815385
303.243397	8000.005538	9.461184	-0.061279	4.815392
303.210273	7999.915197	9.466189	-0.061273	4.815365
303.250711	7999.975706	9.471194	-0.061280	4.815383
303.312211	7999.999156	9.476199	-0.061292	4.815390
303.441112	8000.002345	9.481203	-0.061316	4.815390
303.490752	7999.986053	9.486208	-0.061325	4.815385
303.405542	7999.956840	9.491213	-0.061309	4.815377
303.481529	7999.928158	9.496218	-0.061323	4.815368
303.593450	8000.036879	9.501223	-0.061343	4.815399
303.439017	7999.972318	9.506227	-0.061314	4.815381
303.409951	8000.040227	9.511232	-0.061309	4.815401
303.349104	7999.951564	9.516237	-0.061297	4.815375
303.545450	7999.959076	9.521242	-0.061334	4.815377
303.477680	8000.014588	9.526247	-0.061321	4.815393
303.394128	7999.990747	9.531251	-0.061305	4.815387
303.636824	8000.011853	9.536256	-0.061350	4.815392
303.715119	7999.952213	9.541261	-0.061365	4.815374
303.758244	8000.001011	9.546266	-0.061373	4.815388
303.798143	7999.961043	9.551271	-0.061380	4.815376
303.806444	7999.966511	9.556275	-0.061381	4.815378
303.499782	8000.019137	9.561280	-0.061324	4.815395
303.480322	7999.969636	9.566285	-0.061320	4.815380
303.731910	8000.040055	9.571290	-0.061367	4.815399
303.603584	8000.016540	9.576295	-0.061343	4.815393
303.520458	7999.975604	9.581299	-0.061327	4.815382
303.625127	8000.053210	9.586304	-0.061347	4.815404
303.638986	8000.020293	9.591309	-0.061349	4.815394
303.761745	8000.041551	9.596314	-0.061372	4.815400
303.723128	8000.016316	9.601319	-0.061365	4.815393
303.709642	7999.996840	9.606323	-0.061362	4.815387
303.966727	8000.068420	9.611328	-0.061410	4.815407
303.769466	8000.039488	9.616333	-0.061373	4.815399
303.916031	8000.010906	9.621338	-0.061400	4.815390
303.817786	8000.060570	9.626343	-0.061381	4.815405
303.637699	8000.065056	9.631347	-0.061348	4.815407
303.837653	8000.007431	9.636352	-0.061385	4.815390
303.698081	7999.911050	9.641357	-0.061359	4.815362
303.858429	7999.941481	9.646362	-0.061388	4.815370
303.782519	8000.047093	9.651367	-0.061374	4.815401
304.079341	7999.970765	9.656371	-0.061429	4.815378
303.903453	8000.122819	9.661376	-0.061396	4.815423
303.759843	8000.102257	9.666381	-0.061369	4.815418
303.941384	8000.035776	9.671386	-0.061403	4.815397
304.052373	8000.014087	9.676391	-0.061424	4.815390
303.896907	7999.952714	9.681395	-0.061394	4.815373
304.054422	8000.051503	9.686400	-0.061424	4.815401
304.043061	8000.038476	9.691405	-0.061421	4.815398
304.159286	7999.988015	9.696410	-0.061443	4.815382
303.971127	8000.053291	9.701415	-0.061408	4.815402
303.982568	7999.962616	9.706419	-0.061410	4.815376
304.128272	8000.022733	9.711424	-0.061437	4.815393
304.050704	8000.078083	9.716429	-0.061422	4.815409
304.342268	8000.089312	9.721434	-0.061476	4.815411
304.393226	8000.115795	9.726439	-0.061486	4.815419
304.299910	8000.014834	9.731443	-0.061468	4.815390
304.066860	8000.121051	9.736448	-0.061425	4.815422
304.115767	7999.992519	9.741453	-0.061433	4.815384
304.136295	8000.000327	9.746458	-0.061437	4.815386
304.084931	7999.994119	9.751463	-0.061427	4.815385
304.149309	7999.981277	9.756467	-0.061439	4.815380
304.291001	8000.027433	9.761472	-0.061466	4.815393
304.318123	7999.992597	9.766477	-0.061470	4.815383
304.310819	8000.010633	9.771482	-0.061469	4.815388
304.211508	8000.005769	9.776487	-0.061450	4.815387
304.084380	8000.021820	9.781491	-0.061426	4.815393
304.102228	8000.076613	9.786496	-0.061430	4.815409
304.191089	8000.067383	9.791501	-0.061446	4.815405
304.163635	8000.041263	9.796506	-0.061441	4.815398
304.080649	8000.073009	9.801511	-0.061425	4.815408
304.134727	8000.031138	9.806515	-0.061435	4.815395
304.166269	8000.043404	9.811520	-0.061441	4.815399
304.250811	8000.010589	9.816525	-0.061456	4.815389
304.289033	8000.037929	9.821530	-0.061463	4.815396
304.322308	8000.019228	9.826535	-0.061469	4.815391
304.319704	7999.936871	9.831539	-0.061469	4.815367
304.451584	8000.061959	9.836544	-0.061493	4.815403
304.478829	8000.014299	9.841549	-0.061498	4.815389
304.562592	7999.994296	9.846554	-0.061514	4.815382
304.420539	8000.052854	9.851559	-0.061487	4.815400
304.490048	8000.033684	9.856563	-0.061500	4.815394
304.567000	8000.058460	9.861568	-0.061514	4.815401
304.355713	8000.039983	9.866573	-0.061474	4.815397
304.470040	8000.030106	9.871578	-0.061496	4.815393
304.545458	8000.044168	9.876583	-0.061509	4.815397
304.441645	7999.940896	9.881587	-0.061490	4.815367
304.528088	8000.045992	9.886592	-0.061506	4.815398
304.508988	8000.028560	9.891597	-0.061502	4.815393
304.795125	8000.048251	9.896602	-0.061555	4.815397
304.626995	8000.049728	9.901607	-0.061524	4.815398
304.663267	8000.012906	9.906611	-0.061530	4.815387
304.827096	8000.036983	9.911616	-0.061561	4.815394
304.703264	7999.986821	9.916621	-0.061538	4.815380
304.902758	7999.985837	9.921626	-0.061575	4.815378
304.752887	8000.025026	9.926631	-0.061547	4.815390
304.659956	8000.023473	9.931635	-0.061529	4.815390
304.744240	8000.049439	9.936640	-0.061545	4.815398
304.735517	7999.963774	9.941645	-0.061543	4.815373
304.764627	8000.034787	9.946650	-0.061548	4.815393
304.844416	8000.020062	9.951655	-0.061563	4.815389
304.636272	8000.016601	9.956659	-0.061524	4.815389
304.681979	8000.076132	9.961664	-0.061532	4.815406
304.817174	8000.054843	9.966669	-0.061557	4.815399
304.681382	8000.031204	9.971674	-0.061532	4.815393
304.747148	8000.078240	9.976679	-0.061544	4.815406
304.711267	7999.989987	9.981683	-0.061537	4.815380
304.884376	8000.049490	9.986688	-0.061569	4.815397
305.014826	8000.066602	9.991693	-0.061593	4.815401
305.058258	8000.035243	9.996698	-0.061601	4.815392
304.920441	8000.081045	10.001703	-0.061576	4.815406
304.827365	8000.053837	10.006707	-0.061558	4.815399
305.029197	8000.110611	10.011712	-0.061596	4.815414
305.032577	8000.047591	10.016717	-0.061596	4.815396
304.911908	7999.977172	10.021722	-0.061573	4.815376
304.964131	7999.986574	10.026727	-0.061583	4.815378
305.037385	8000.034804	10.031731	-0.061596	4.815392
305.055732	8000.074643	10.036736	-0.061600	4.815404
304.775187	8000.007988	10.041741	-0.061547	4.815385
304.890144	8000.013086	10.046746	-0.061569	4.815386
304.730082	8000.052106	10.051751	-0.061539	4.815399
304.771792	8000.033544	10.056755	-0.061546	4.815393
305.118276	8000.034996	10.061760	-0.061611	4.815392
305.034219	8000.020764	10.066765	-0.061595	4.815388
304.925525	7999.994366	10.071770	-0.061574	4.815381
304.973216	8000.078513	10.076775	-0.061583	4.815405
305.031426	8000.061294	10.081779	-0.061594	4.815400
305.123063	8000.067074	10.086784	-0.061611	4.815401
305.013730	8000.036391	10.091789	-0.061590	4.815393
305.216131	8000.020491	10.096794	-0.061628	4.815387
305.284240	8000.109253	10.101799	-0.061640	4.815413
305.085071	8000.026844	10.106803	-0.061603	4.815390
305.152936	8000.102775	10.111808	-0.061616	4.815411
305.175321	8000.074274	10.116813	-0.061620	4.815403
304.920838	8000.001638	10.121818	-0.061572	4.815383
304.901798	8000.086817	10.126823	-0.061568	4.815408
304.859603	8000.050832	10.131827	-0.061560	4.815398
305.012953	8000.127111	10.136832	-0.061589	4.815419
304.839059	8000.076118	10.141837	-0.061556	4.815405
305.002323	8000.067052	10.146842	-0.061586	4.815402
305.025163	8000.042834	10.151847	-0.061591	4.815395
304.965335	8000.000144	10.156851	-0.061579	4.815382
305.068461	8000.061695	10.161856	-0.061598	4.815400
305.140316	8000.060735	10.166861	-0.061612	4.815399
305.201026	7999.995458	10.171866	-0.061623	4.815380
305.174142	8000.076232	10.176871	-0.061618	4.815404
305.000061	7999.966450	10.181875	-0.061585	4.815372
304.991616	8000.078526	10.186880	-0.061583	4.815405
305.054519	8000.045351	10.191885	-0.061595	4.815395
305.130337	8000.027355	10.196890	-0.061609	4.815390
304.980998	8000.101825	10.201895	-0.061581	4.815412
304.779717	8000.001212	10.206899	-0.061543	4.815384
304.902619	8000.026749	10.211904	-0.061566	4.815390
304.952569	7999.929229	10.216909	-0.061575	4.815362
304.950987	7999.921708	10.221914	-0.061575	4.815360
304.963874	8000.039481	10.226919	-0.061577	4.815394
305.045369	7999.948897	10.231923	-0.061592	4.815367
305.384473	8000.052837	10.236928	-0.061655	4.815396
305.286745	8000.022345	10.241933	-0.061637	4.815387
305.284788	8000.016955	10.246938	-0.061636	4.815386
305.236116	8000.072785	10.251943	-0.061627	4.815402
305.124653	8000.006793	10.256947	-0.061606	4.815384
305.071991	8000.094622	10.261952	-0.061596	4.815409
305.070708	8000.031525	10.266957	-0.061596	4.815391
305.148072	8000.050964	10.271962	-0.061610	4.815396
305.024024	8000.085237	10.276967	-0.061587	4.815407
305.033227	8000.094996	10.281971	-0.061588	4.815410
305.256485	8000.078373	10.286976	-0.061630	4.815404
305.102093	8000.054425	10.291981	-0.061601	4.815398
305.268155	8000.016546	10.296986	-0.061631	4.815386
305.196796	8000.109410	10.301991	-0.061618	4.815413
305.065697	8000.092261	10.306995	-0.061594	4.815409
305.298071	8000.083272	10.312000	-0.061637	4.815405
305.345777	8000.088324	10.317005	-0.061645	4.815406
305.296954	8000.097122	10.322010	-0.061636	4.815409
305.225079	7999.933451	10.327015	-0.061622	4.815362
305.382724	7999.890089	10.332019	-0.061652	4.815348
305.416126	8000.037062	10.337024	-0.061658	4.815391
305.439042	7999.991468	10.342029	-0.061662	4.815378
305.531847	7999.978028	10.347034	-0.061679	4.815373
305.639861	8000.005457	10.352039	-0.061699	4.815381
305.559681	8000.006253	10.357043	-0.061684	4.815381
305.527150	8000.046318	10.362048	-0.061678	4.815393
305.394288	8000.016312	10.367053	-0.061653	4.815385
305.517163	7999.996958	10.372058	-0.061676	4.815379
305.578917	8000.067444	10.377063	-0.061687	4.815399
305.313874	7999.995701	10.382067	-0.061637	4.815380
305.579889	8000.090949	10.387072	-0.061687	4.815406
305.503051	8000.087525	10.392077	-0.061672	4.815405
305.616091	8000.071214	10.397082	-0.061693	4.815400
305.651547	8000.132714	10.402087	-0.061700	4.815418
305.354083	8000.049744	10.407091	-0.061644	4.815395
305.564168	8000.129101	10.412096	-0.061683	4.815417
305.587331	8000.095268	10.417101	-0.061687	4.815407
305.610273	8000.094566	10.422106	-0.061691	4.815407
305.456925	8000.131560	10.427111	-0.061663	4.815419
305.595200	8000.076119	10.432115	-0.061688	4.815402
305.595175	8000.147720	10.437120	-0.061688	4.815423
305.470213	8000.061195	10.442125	-0.061665	4.815398
305.486426	8000.051830	10.447130	-0.061668	4.815395
305.553401	8000.142712	10.452135	-0.061680	4.815421
305.328151	8000.086591	10.457139	-0.061638	4.815406
305.467687	8000.060031	10.462144	-0.061664	4.815398
305.518349	8000.021309	10.467149	-0.061673	4.815386
305.505281	8000.016804	10.472154	-0.061670	4.815385
305.427006	8000.049697	10.477159	-0.061656	4.815395
305.465509	7999.966951	10.482163	-0.061663	4.815370
305.579126	8000.070362	10.487168	-0.061684	4.815400
305.588202	8000.019193	10.492173	-0.061685	4.815385
305.645596	8000.070368	10.497178	-0.061696	4.815400
305.802224	8000.063331	10.502183	-0.061725	4.815397
305.494664	8000.103113	10.507187	-0.061667	4.815410
305.529177	8000.172079	10.512192	-0.061674	4.815430
305.566392	8000.097862	10.517197	-0.061680	4.815408
305.703433	8000.058434	10.522202	-0.061706	4.815396
305.625666	8000.095611	10.527207	-0.061691	4.815407
305.653537	8000.034065	10.532211	-0.061696	4.815389
305.770125	8000.104392	10.537216	-0.061718	4.815409
305.520291	8000.013660	10.542221	-0.061671	4.815384
305.505206	8000.046531	10.547226	-0.061668	4.815394
305.621528	8000.058066	10.552231	-0.061690	4.815396
305.576534	8000.043411	10.557235	-0.061681	4.815392
305.466112	8000.091805	10.562240	-0.061660	4.815407
305.710795	8000.076607	10.567245	-0.061706	4.815401
305.948113	7999.965088	10.572250	-0.061750	4.815368
305.781611	8000.047826	10.577255	-0.061719	4.815393
305.544164	8000.025707	10.582259	-0.061674	4.815387
305.646160	8000.095791	10.587264	-0.061693	4.815407
305.664690	8000.015920	10.592269	-0.061696	4.815384
305.575487	8000.072147	10.597274	-0.061680	4.815401
305.689811	8000.033411	10.602279	-0.061701	4.815389
305.672742	7999.989292	10.607283	-0.061698	4.815376
305.730541	8000.112087	10.612288	-0.061708	4.815412
305.682497	8000.025768	10.617293	-0.061699	4.815387
305.734585	7999.998827	10.622298	-0.061709	4.815379
305.799591	8000.098228	10.627303	-0.061721	4.815407
305.757258	7999.989557	10.632307	-0.061713	4.815376
305.814473	8000.047142	10.637312	-0.061723	4.815392
305.577112	8000.037851	10.642317	-0.061679	4.815391
305.770232	7999.971561	10.647322	-0.061714	4.815370
305.820947	8000.097446	10.652327	-0.061724	4.815407
305.795159	8000.052113	10.657331	-0.061719	4.815394
305.704249	8000.049524	10.662336	-0.061702	4.815394
305.984021	8000.031701	10.667341	-0.061754	4.815387
306.089876	8000.062302	10.672346	-0.061773	4.815395
305.857129	8000.081946	10.677351	-0.061730	4.815402
305.704930	8000.067653	10.682355	-0.061701	4.815399
305.680194	8000.103572	10.687360	-0.061697	4.815409
305.750698	8000.091900	10.692365	-0.061710	4.815406
305.802453	8000.092745	10.697370	-0.061719	4.815406
305.762743	8000.132691	10.702375	-0.061712	4.815418
305.650921	8000.027144	10.707379	-0.061690	4.815387
305.648718	8000.062366	10.712384	-0.061690	4.815398
305.685948	8000.036248	10.717389	-0.061697	4.815390
305.859211	8000.022004	10.722394	-0.061729	4.815385
305.762209	8000.053519	10.727399	-0.061711	4.815395
305.813050	7999.970976	10.732403	-0.061720	4.815370
305.977567	8000.052786	10.737408	-0.061750	4.815393
305.880322	8000.041541	10.742413	-0.061732	4.815390
306.010645	7999.967797	10.747418	-0.061756	4.815368
305.793044	8000.061445	10.752423	-0.061716	4.815397
305.878345	7999.991231	10.757427	-0.061731	4.815376
306.053464	8000.052908	10.762432	-0.061764	4.815393
305.780120	8000.047296	10.767437	-0.061713	4.815393
305.974146	8000.044085	10.772442	-0.061749	4.815391
305.910152	8000.038736	10.777447	-0.061737	4.815390
305.660396	7999.977933	10.782451	-0.061690	4.815373
305.661161	8000.078406	10.787456	-0.061690	4.815402
305.495770	8000.060688	10.792461	-0.061659	4.815398
305.594896	8000.015287	10.797466	-0.061677	4.815384
305.757179	8000.099197	10.802471	-0.061707	4.815408
305.892988	8000.014856	10.807475	-0.061733	4.815383
305.842002	8000.005447	10.812480	-0.061723	4.815380
305.612365	7999.989871	10.817485	-0.061680	4.815377
305.768990	8000.028794	10.822490	-0.061709	4.815387
305.773493	8000.056646	10.827495	-0.061710	4.815395
305.758191	7999.964457	10.832499	-0.061707	4.815369
305.809115	7999.978114	10.837504	-0.061716	4.815372
305.637669	8000.006257	10.842509	-0.061684	4.815381
305.645278	7999.970028	10.847514	-0.061685	4.815371
305.889639	7999.971926	10.852519	-0.061731	4.815370
305.900961	8000.005236	10.857523	-0.061733	4.815380
306.003856	8000.080680	10.862528	-0.061752	4.815401
305.914233	8000.032151	10.867533	-0.061735	4.815388
305.983065	8000.064276	10.872538	-0.061747	4.815397
306.365326	8000.113354	10.877543	-0.061819	4.815409
306.174872	8000.040706	10.882547	-0.061783	4.815389
306.143602	8000.034830	10.887552	-0.061777	4.815387
305.967998	8000.068248	10.892557	-0.061744	4.815398
306.031032	8000.012629	10.897562	-0.061756	4.815381
305.996034	8000.091133	10.902567	-0.061749	4.815404
305.883688	8000.000541	10.907571	-0.061728	4.815379
306.091142	8000.015723	10.912576	-0.061766	4.815382
305.953374	8000.002738	10.917581	-0.061741	4.815379
306.147500	7999.963187	10.922586	-0.061777	4.815366
306.105721	7999.995616	10.927591	-0.061769	4.815376
306.017791	7999.980251	10.932595	-0.061752	4.815372
306.055272	8000.017200	10.937600	-0.061759	4.815383
306.190673	7999.989502	10.942605	-0.061784	4.815374
306.050019	8000.014949	10.947610	-0.061758	4.815382
306.016908	8000.093484	10.952615	-0.061751	4.815405
306.030849	8000.007122	10.957619	-0.061754	4.815380
306.279971	8000.063613	10.962624	-0.061800	4.815395
306.135212	8000.034478	10.967629	-0.061773	4.815387
306.014142	7999.981153	10.972634	-0.061750	4.815372
306.131662	8000.009809	10.977639	-0.061772	4.815380
306.011640	8000.053768	10.982643	-0.061749	4.815394
306.080670	8000.021764	10.987648	-0.061762	4.815384
306.214518	8000.018624	10.992653	-0.061787	4.815382
306.341401	7999.976890	10.997658	-0.061810	4.815370
306.302829	8000.080988	11.002663	-0.061803	4.815400
306.191142	8000.064159	11.007667	-0.061782	4.815396
306.155863	8000.073181	11.012672	-0.061775	4.815399
306.059759	8000.035233	11.017677	-0.061757	4.815388
306.067818	8000.057799	11.022682	-0.061759	4.815395
306.308975	8000.091712	11.027687	-0.061804	4.815403
306.067262	8000.038524	11.032691	-0.061758	4.815389
306.331959	8000.098480	11.037696	-0.061808	4.815405
306.194423	8000.071602	11.042701	-0.061782	4.815398
306.093675	8000.020751	11.047706	-0.061763	4.815384
306.037948	8000.033709	11.052711	-0.061752	4.815388
306.053734	7999.989065	11.057715	-0.061755	4.815375
306.400873	8000.050387	11.062720	-0.061820	4.815391
306.285559	8000.021740	11.067725	-0.061798	4.815383
306.234952	8000.039059	11.072730	-0.061788	4.815388
306.282717	8000.071904	11.077735	-0.061797	4.815398
306.162819	8000.013253	11.082739	-0.061775	4.815381
306.324394	8000.037295	11.087744	-0.061805	4.815387
306.240057	8000.028402	11.092749	-0.061789	4.815385
306.335807	8000.026769	11.097754	-0.061806	4.815384
306.229116	8000.019643	11.102759	-0.061786	4.815383
306.328646	8000.068310	11.107763	-0.061805	4.815396
306.360382	8000.062410	11.112768	-0.061811	4.815395
306.202888	8000.004204	11.117773	-0.061781	4.815378
306.228378	7999.986442	11.122778	-0.061786	4.815373
306.225973	8000.071899	11.127783	-0.061785	4.815398
306.116108	8000.043343	11.132787	-0.061764	4.815390
306.174356	8000.045364	11.137792	-0.061775	4.815390
306.298305	8000.026028	11.142797	-0.061798	4.815384
306.261833	8000.009377	11.147802	-0.061791	4.815380
306.168240	8000.069807	11.152807	-0.061774	4.815398
306.197967	8000.016843	11.157811	-0.061779	4.815382
306.359101	8000.017362	11.162816	-0.061809	4.815381
306.272649	8000.058671	11.167821	-0.061793	4.815394
306.162219	8000.019417	11.172826	-0.061772	4.815383
306.376708	8000.082816	11.177831	-0.061812	4.815400
306.125949	8000.016651	11.182835	-0.061765	4.815382
306.336730	8000.031889	11.187840	-0.061804	4.815386
306.249929	8000.015473	11.192845	-0.061788	4.815381
306.455156	7999.993208	11.197850	-0.061826	4.815374
306.522588	8000.095857	11.202855	-0.061838	4.815404
306.182797	8000.039974	11.207859	-0.061775	4.815389
306.379750	8000.053914	11.212864	-0.061811	4.815392
306.290970	8000.056704	11.217869	-0.061794	4.815393
306.288014	8000.029920	11.222874	-0.061794	4.815385
306.408502	8000.041524	11.227879	-0.061816	4.815388
306.426582	7999.977677	11.232883	-0.061819	4.815370
306.313585	8000.065577	11.237888	-0.061798	4.815396
306.240100	8000.069690	11.242893	-0.061784	4.815397
306.240240	8000.041888	11.247898	-0.061784	4.815389
306.354852	8000.048050	11.252903	-0.061805	4.815390
306.233502	8000.029992	11.257907	-0.061783	4.815386
306.546858	8000.095031	11.262912	-0.061841	4.815403
306.387878	8000.102002	11.267917	-0.061811	4.815406
306.288379	7999.985969	11.272922	-0.061792	4.815373
306.208544	8000.068005	11.277927	-0.061777	4.815397
306.433744	8000.020418	11.282931	-0.061819	4.815382
306.576349	8000.052698	11.287936	-0.061846	4.815391
306.566560	8000.077107	11.292941	-0.061844	4.815398
306.438608	8000.006564	11.297946	-0.061820	4.815378
306.403752	8000.036970	11.302951	-0.061813	4.815387
306.402919	8000.025185	11.307955	-0.061813	4.815384
306.545917	7999.997614	11.312960	-0.061839	4.815375
306.499078	8000.075921	11.317965	-0.061830	4.815398
306.579540	8000.033418	11.322970	-0.061845	4.815385
306.521935	8000.059172	11.327975	-0.061834	4.815393
306.579142	8000.036591	11.332979	-0.061845	4.815386
306.584102	8000.053762	11.337984	-0.061845	4.815391
306.417843	8000.059544	11.342989	-0.061814	4.815394
306.546803	8000.008224	11.347994	-0.061838	4.815378
306.543990	8000.030611	11.352999	-0.061838	4.815385
306.362854	7999.990184	11.358003	-0.061804	4.815374
306.501860	8000.025610	11.363008	-0.061829	4.815383
306.491124	8000.058554	11.368013	-0.061827	4.815393
306.552743	7999.995429	11.373018	-0.061839	4.815374
306.627293	8000.055441	11.378023	-0.061852	4.815391
306.478941	8000.004868	11.383027	-0.061825	4.815377
306.627796	8000.040458	11.388032	-0.061852	4.815387
306.527733	8000.033442	11.393037	-0.061833	4.815385
306.679222	8000.057317	11.398042	-0.061861	4.815392
306.826019	8000.059738	11.403047	-0.061889	4.815392
306.464036	8000.004555	11.408051	-0.061821	4.815377
306.458517	7999.984141	11.413056	-0.061820	4.815371
306.700487	7999.950728	11.418061	-0.061865	4.815360
306.764726	7999.999879	11.423066	-0.061877	4.815375
306.595773	8000.079370	11.428071	-0.061845	4.815399
306.444375	8000.000956	11.433075	-0.061817	4.815376
306.611077	8000.027221	11.438080	-0.061847	4.815383
306.731932	8000.068760	11.443085	-0.061870	4.815395
306.815953	8000.019902	11.448090	-0.061885	4.815380
306.771614	8000.095045	11.453095	-0.061877	4.815402
306.625965	7999.983591	11.458099	-0.061850	4.815370
306.718961	8000.087732	11.463104	-0.061867	4.815400
306.623426	8000.096824	11.468109	-0.061849	4.815404
306.643998	8000.054396	11.473114	-0.061853	4.815391
306.856916	8000.087842	11.478119	-0.061892	4.815400
306.740259	8000.053828	11.483123	-0.061870	4.815390
306.745746	8000.062456	11.488128	-0.061871	4.815393
306.821736	8000.077599	11.493133	-0.061885	4.815397
306.638423	8000.030722	11.498138	-0.061851	4.815384
306.909404	8000.099335	11.503143	-0.061901	4.815403
306.768418	8000.040332	11.508147	-0.061875	4.815386
306.923111	8000.039677	11.513152	-0.061903	4.815385
306.820727	8000.051862	11.518157	-0.061884	4.815390
306.691776	8000.019782	11.523162	-0.061860	4.815381
306.654862	8000.136735	11.528167	-0.061853	4.815415
306.505713	8000.089355	11.533171	-0.061825	4.815402
306.604723	8000.114499	11.538176	-0.061843	4.815409
306.633443	8000.064724	11.543181	-0.061849	4.815394
306.719504	7999.979557	11.548186	-0.061864	4.815369
306.848835	8000.114231	11.553191	-0.061888	4.815408
306.669250	8000.125136	11.558195	-0.061855	4.815412
306.717352	8000.069269	11.563200	-0.061864	4.815395
306.774641	8000.068067	11.568205	-0.061874	4.815395
306.854883	7999.991355	11.573210	-0.061889	4.815372
306.881747	8000.105090	11.578215	-0.061894	4.815405
306.717030	8000.074555	11.583219	-0.061863	4.815397
306.562911	8000.047402	11.588224	-0.061834	4.815390
306.470789	8000.017002	11.593229	-0.061817	4.815381
306.613316	7999.952011	11.598234	-0.061843	4.815361
306.789782	8000.055399	11.603239	-0.061876	4.815391
306.490548	8000.066458	11.608243	-0.061820	4.815395
306.623184	8000.042990	11.613248	-0.061845	4.815388
306.587370	8000.092621	11.618253	-0.061838	4.815403
306.788476	8000.064944	11.623258	-0.061875	4.815394
306.811939	8000.087766	11.628263	-0.061879	4.815400
306.665649	8000.001954	11.633267	-0.061852	4.815376
306.795455	8000.015850	11.638272	-0.061876	4.815379
306.680662	8000.093032	11.643277	-0.061854	4.815402
306.735826	7999.988113	11.648282	-0.061864	4.815371
306.975947	8000.086143	11.653287	-0.061909	4.815399
306.803262	8000.019133	11.658291	-0.061877	4.815380
306.709927	8000.050708	11.663296	-0.061859	4.815390
306.783336	8000.085048	11.668301	-0.061873	4.815399
306.941228	8000.031001	11.673306	-0.061902	4.815383
306.705559	8000.017461	11.678311	-0.061858	4.815380
306.604796	7999.933473	11.683315	-0.061839	4.815356
306.898583	8000.005669	11.688320	-0.061894	4.815376
306.696382	8000.033302	11.693325	-0.061856	4.815385
306.652817	7999.976984	11.698330	-0.061847	4.815369
306.844197	8000.041070	11.703335	-0.061883	4.815386
306.792112	8000.039125	11.708339	-0.061873	4.815386
306.858450	8000.042349	11.713344	-0.061885	4.815387
306.776205	8000.086934	11.718349	-0.061870	4.815400
306.844740	8000.053853	11.723354	-0.061882	4.815390
306.788946	8000.115979	11.728359	-0.061872	4.815409
306.940941	8000.070386	11.733363	-0.061900	4.815395
306.902997	8000.129602	11.738368	-0.061893	4.815412
306.843715	8000.102952	11.743373	-0.061882	4.815404
306.837563	8000.008774	11.748378	-0.061880	4.815377
307.193108	8000.101236	11.753383	-0.061946	4.815402
306.750644	8000.008375	11.758387	-0.061864	4.815377
306.945497	8000.075726	11.763392	-0.061900	4.815396
306.948645	8000.078972	11.768397	-0.061901	4.815397
306.869644	8000.019928	11.773402	-0.061886	4.815380
306.813670	8000.095947	11.778407	-0.061875	4.815403
306.852323	8000.015339	11.783411	-0.061882	4.815379
306.899201	8000.017172	11.788416	-0.061891	4.815379
306.885179	8000.038304	11.793421	-0.061888	4.815385
306.884136	8000.056444	11.798426	-0.061888	4.815391
307.080886	8000.105656	11.803431	-0.061924	4.815404
306.899643	8000.013919	11.808435	-0.061890	4.815378
306.872822	8000.084008	11.813440	-0.061885	4.815399
306.921493	8000.022806	11.818445	-0.061894	4.815381
306.882460	7999.996492	11.823450	-0.061886	4.815373
306.861560	8000.074162	11.828455	-0.061883	4.815396
306.676525	8000.047565	11.833459	-0.061848	4.815389
306.991030	8000.061317	11.838464	-0.061906	4.815392
306.866039	8000.095574	11.843469	-0.061883	4.815402
306.844431	8000.060998	11.848474	-0.061879	4.815392
306.776785	8000.103687	11.853479	-0.061866	4.815405
306.818704	8000.047718	11.858483	-0.061874	4.815389
306.840927	8000.042728	11.863488	-0.061878	4.815387
306.951441	8000.037065	11.868493	-0.061898	4.815385
307.034015	8000.042696	11.873498	-0.061913	4.815386
306.920179	8000.085689	11.878503	-0.061892	4.815399
306.843884	8000.024553	11.883507	-0.061878	4.815382
306.937778	8000.044268	11.888512	-0.061895	4.815387
307.043274	8000.080208	11.893517	-0.061914	4.815397
306.863194	8000.007731	11.898522	-0.061881	4.815377
307.024421	8000.041389	11.903527	-0.061911	4.815386
306.853436	7999.990440	11.908531	-0.061879	4.815372
307.042237	8000.065173	11.913536	-0.061914	4.815393
306.822286	8000.059375	11.918541	-0.061872	4.815392
307.031569	8000.023283	11.923546	-0.061911	4.815380
307.043408	8000.058739	11.928551	-0.061913	4.815391
306.936151	8000.040914	11.933555	-0.061893	4.815386
306.939453	8000.052714	11.938560	-0.061894	4.815390
306.896293	8000.038089	11.943565	-0.061886	4.815385
306.829600	8000.017730	11.948570	-0.061873	4.815380
307.152436	8000.098961	11.953575	-0.061933	4.815402
307.134458	7999.992829	11.958579	-0.061929	4.815371
307.110501	8000.053345	11.963584	-0.061925	4.815389
306.937846	8000.037643	11.968589	-0.061893	4.815385
307.012268	7999.991832	11.973594	-0.061906	4.815371
307.118808	8000.066270	11.978599	-0.061926	4.815393
306.923702	8000.012784	11.983603	-0.061889	4.815378
307.115471	7999.988158	11.988608	-0.061925	4.815370
307.158039	8000.031607	11.993613	-0.061933	4.815382
307.104774	7999.984748	11.998618	-0.061923	4.815369
307.118622	8000.082234	12.003623	-0.061925	4.815397
306.941525	8000.040804	12.008627	-0.061892	4.815386
306.891344	8000.033545	12.013632	-0.061883	4.815384
307.051808	8000.098189	12.018637	-0.061912	4.815402
306.941187	8000.023656	12.023642	-0.061891	4.815381
307.047237	8000.051055	12.028647	-0.061911	4.815389
306.815407	8000.018338	12.033651	-0.061868	4.815380
306.764545	8000.018550	12.038656	-0.061858	4.815380
306.985426	8000.067092	12.043661	-0.061899	4.815394
306.985416	8000.082043	12.048666	-0.061899	4.815398
306.963550	8000.091288	12.053671	-0.061895	4.815401
307.117072	8000.036099	12.058675	-0.061923	4.815384
307.198638	8000.059885	12.063680	-0.061938	4.815390
307.040302	8000.107485	12.068685	-0.061909	4.815405
306.867520	8000.030853	12.073690	-0.061876	4.815384
307.007146	8000.090875	12.078695	-0.061902	4.815400
306.862470	8000.060672	12.083699	-0.061875	4.815392
306.902238	8000.073076	12.088704	-0.061882	4.815396
306.948970	8000.086664	12.093709	-0.061891	4.815399
307.091163	8000.004565	12.098714	-0.061917	4.815375
307.164422	8000.051729	12.103719	-0.061931	4.815388
307.104305	8000.031479	12.108723	-0.061919	4.815383
306.978179	8000.015479	12.113728	-0.061896	4.815379
307.010784	8000.090829	12.118733	-0.061902	4.815400
306.988675	7999.989973	12.123738	-0.061897	4.815371
307.048457	8000.047602	12.128743	-0.061908	4.815388
306.978509	7999.991916	12.133747	-0.061895	4.815372
306.902670	8000.054779	12.138752	-0.061881	4.815390
306.984083	8000.062529	12.143757	-0.061896	4.815392
306.911702	8000.095520	12.148762	-0.061882	4.815402
306.939962	8000.132318	12.153767	-0.061887	4.815413
307.113165	8000.090282	12.158771	-0.061920	4.815400
307.035642	8000.080433	12.163776	-0.061905	4.815397
307.102831	8000.065500	12.168781	-0.061917	4.815393
306.859216	8000.039001	12.173786	-0.061872	4.815386
307.060540	8000.084012	12.178791	-0.061909	4.815398
307.181098	8000.037897	12.183795	-0.061931	4.815384
307.143035	8000.034046	12.188800	-0.061924	4.815383
306.928919	8000.023001	12.193805	-0.061884	4.815381
306.925327	7999.953450	12.198810	-0.061883	4.815361
306.924164	8000.103063	12.203815	-0.061883	4.815404
307.040475	8000.072911	12.208819	-0.061904	4.815395
307.196182	8000.066928	12.213824	-0.061933	4.815393
307.037655	8000.086733	12.218829	-0.061904	4.815399
306.909198	8000.018319	12.223834	-0.061880	4.815380
307.113800	8000.039869	12.228839	-0.061918	4.815385
306.870324	7999.943894	12.233843	-0.061872	4.815358
306.912075	7999.980915	12.238848	-0.061880	4.815369
307.119914	8000.050619	12.243853	-0.061918	4.815388
306.967057	8000.014936	12.248858	-0.061890	4.815379
307.136162	8000.028415	12.253863	-0.061921	4.815382
307.054410	8000.044149	12.258867	-0.061906	4.815387
307.140423	8000.055181	12.263872	-0.061921	4.815390
306.978022	8000.141194	12.268877	-0.061891	4.815415
306.860175	8000.095402	12.273882	-0.061869	4.815403
306.924343	8000.142415	12.278887	-0.061881	4.815416
306.831046	8000.066033	12.283891	-0.061863	4.815394
306.787680	8000.035371	12.288896	-0.061855	4.815385
306.816516	8000.079661	12.293901	-0.061860	4.815398
306.828665	8000.011440	12.298906	-0.061862	4.815378
307.058677	7999.995999	12.303911	-0.061905	4.815373
307.191302	8000.020632	12.308915	-0.061930	4.815379
307.202814	8000.059290	12.313920	-0.061932	4.815390
306.885796	8000.076467	12.318925	-0.061872	4.815397
306.909970	7999.993481	12.323930	-0.061877	4.815373
307.125933	7999.987428	12.328935	-0.061917	4.815370
307.128528	7999.991733	12.333939	-0.061917	4.815371
307.060862	7999.964945	12.338944	-0.061904	4.815364
306.931354	8000.069674	12.343949	-0.061880	4.815395
306.928582	7999.968070	12.348954	-0.061879	4.815365
307.083525	8000.052930	12.353959	-0.061908	4.815389
306.899307	8000.047725	12.358963	-0.061874	4.815389
306.936724	8000.020541	12.363968	-0.061880	4.815380
307.004639	8000.060133	12.368973	-0.061893	4.815392
306.857911	7999.949730	12.373978	-0.061865	4.815360
307.074822	8000.002481	12.378983	-0.061906	4.815375
307.300688	7999.974145	12.383987	-0.061948	4.815365
306.978352	7999.938860	12.388992	-0.061887	4.815356
307.003988	8000.006611	12.393997	-0.061892	4.815376
307.089724	7999.977022	12.399002	-0.061908	4.815367
307.049737	8000.066132	12.404007	-0.061900	4.815393
307.064607	8000.006508	12.409011	-0.061903	4.815376
307.087425	7999.996184	12.414016	-0.061907	4.815373
307.084114	7999.996115	12.419021	-0.061906	4.815373
306.805785	7999.947664	12.424026	-0.061854	4.815360
307.324700	8000.078107	12.429031	-0.061951	4.815395
307.189477	8000.056612	12.434035	-0.061925	4.815390
307.028824	8000.002628	12.439040	-0.061895	4.815375
307.182245	8000.006227	12.444045	-0.061924	4.815375
307.161112	7999.963108	12.449050	-0.061920	4.815363
307.120441	7999.993418	12.454055	-0.061912	4.815372
307.081585	8000.029103	12.459059	-0.061905	4.815382
307.187900	8000.055437	12.464064	-0.061924	4.815390
307.293178	7999.951348	12.469069	-0.061944	4.815359
307.137794	7999.918830	12.474074	-0.061915	4.815350
307.283858	8000.003543	12.479079	-0.061942	4.815374
307.117397	7999.984737	12.484083	-0.061911	4.815369
307.279657	7999.970311	12.489088	-0.061941	4.815364
307.295500	8000.051797	12.494093	-0.061943	4.815388
307.363627	8000.037948	12.499098	-0.061956	4.815384
307.553806	8000.018641	12.504103	-0.061991	4.815377
307.232802	7999.969481	12.509107	-0.061931	4.815364
307.371627	7999.958942	12.514112	-0.061957	4.815360
307.427035	7999.964123	12.519117	-0.061967	4.815362
307.314348	7999.978275	12.524122	-0.061946	4.815366
307.361668	8000.033560	12.529127	-0.061955	4.815382
307.155459	7999.971339	12.534131	-0.061916	4.815365
307.139933	7999.980688	12.539136	-0.061913	4.815368
307.054016	7999.996353	12.544141	-0.061897	4.815373
307.172954	8000.001518	12.549146	-0.061919	4.815374
307.211861	8000.057733	12.554151	-0.061926	4.815390
307.123713	7999.962195	12.559155	-0.061909	4.815363
307.218558	8000.024681	12.564160	-0.061927	4.815380
307.471613	8000.042759	12.569165	-0.061974	4.815385
307.283491	7999.985113	12.574170	-0.061939	4.815369
307.318404	8000.044468	12.579175	-0.061945	4.815386
307.270574	7999.979528	12.584179	-0.061936	4.815367
307.340041	7999.987080	12.589184	-0.061949	4.815369
307.393162	8000.054219	12.594189	-0.061959	4.815388
307.349422	8000.018207	12.599194	-0.061950	4.815378
307.331044	8000.018958	12.604199	-0.061947	4.815378
307.168007	7999.972417	12.609203	-0.061916	4.815365
307.206955	7999.979462	12.614208	-0.061923	4.815367
307.257332	8000.096794	12.619213	-0.061933	4.815401
307.117880	7999.996130	12.624218	-0.061906	4.815373
307.206453	8000.031790	12.629223	-0.061923	4.815383
307.142900	7999.990105	12.634227	-0.061911	4.815371
307.243504	7999.941522	12.639232	-0.061929	4.815356
307.324203	8000.033702	12.644237	-0.061944	4.815383
307.366586	7999.964913	12.649242	-0.061952	4.815362
307.539351	8000.018003	12.654247	-0.061984	4.815377
307.260061	8000.012290	12.659251	-0.061932	4.815377
307.347376	8000.025482	12.664256	-0.061948	4.815380
307.437265	8000.021615	12.669261	-0.061965	4.815379
307.469571	7999.928074	12.674266	-0.061970	4.815351
307.350982	7999.944266	12.679271	-0.061948	4.815356
307.338289	7999.990005	12.684275	-0.061946	4.815370
307.545698	7999.950674	12.689280	-0.061984	4.815357
307.542802	7999.966646	12.694285	-0.061983	4.815362
307.449879	7999.947990	12.699290	-0.061966	4.815357
307.501312	7999.958450	12.704295	-0.061975	4.815360
307.326876	7999.935235	12.709299	-0.061943	4.815354
307.275430	7999.989952	12.714304	-0.061933	4.815370
307.382381	7999.991712	12.719309	-0.061953	4.815370
307.416341	7999.942023	12.724314	-0.061959	4.815355
307.480161	7999.983686	12.729319	-0.061971	4.815367
307.347853	7999.945137	12.734323	-0.061946	4.815357
307.503227	7999.989386	12.739328	-0.061975	4.815369
307.540331	8000.022055	12.744333	-0.061982	4.815378
307.480113	7999.970805	12.749338	-0.061970	4.815364
307.665123	7999.998444	12.754343	-0.062004	4.815371
307.585268	7999.951144	12.759347	-0.061989	4.815357
307.557321	7999.976321	12.764352	-0.061984	4.815365
307.568512	8000.076971	12.769357	-0.061986	4.815394
307.436152	7999.956114	12.774362	-0.061961	4.815360
307.629882	8000.029861	12.779367	-0.061997	4.815380
307.490972	8000.028613	12.784371	-0.061971	4.815380
307.435709	7999.991341	12.789376	-0.061961	4.815370
307.308360	8000.055488	12.794381	-0.061937	4.815389
307.206104	8000.031332	12.799386	-0.061918	4.815383
307.204757	8000.076190	12.804391	-0.061917	4.815396
307.175455	7999.942079	12.809395	-0.061912	4.815357
307.260094	8000.001189	12.814400	-0.061927	4.815374
307.410701	8000.022913	12.819405	-0.061955	4.815379
307.394946	7999.962780	12.824410	-0.061952	4.815362
307.431402	8000.068124	12.829415	-0.061959	4.815392
307.503919	7999.997697	12.834419	-0.061972	4.815371
307.604864	8000.038907	12.839424	-0.061991	4.815383
307.513970	8000.069453	12.844429	-0.061974	4.815392
307.391100	7999.976546	12.849434	-0.061951	4.815366
307.332102	8000.085651	12.854439	-0.061940	4.815398
307.402168	8000.004494	12.859443	-0.061952	4.815374
307.431356	7999.963278	12.864448	-0.061958	4.815362
307.431309	8000.033811	12.869453	-0.061958	4.815382
307.294330	7999.974875	12.874458	-0.061932	4.815366
307.453918	7999.952923	12.879463	-0.061961	4.815359
307.364996	7999.958918	12.884467	-0.061945	4.815361
307.629495	7999.948325	12.889472	-0.061994	4.815356
307.521067	7999.995683	12.894477	-0.061973	4.815371
307.410529	7999.994906	12.899482	-0.061953	4.815371
307.551847	8000.088093	12.904487	-0.061979	4.815398
307.409375	8000.124198	12.909491	-0.061952	4.815409
307.568443	8000.071239	12.914496	-0.061982	4.815393
307.464060	8000.055599	12.919501	-0.061962	4.815389
307.438606	8000.019890	12.924506	-0.061957	4.815378
307.528076	8000.053427	12.929511	-0.061974	4.815388
307.550659	7999.990723	12.934515	-0.061978	4.815369
307.617529	7999.984336	12.939520	-0.061990	4.815367
307.643207	8000.070261	12.944525	-0.061995	4.815392
307.442862	7999.964311	12.949530	-0.061957	4.815362
307.439304	7999.997375	12.954535	-0.061956	4.815372
307.493674	7999.984367	12.959539	-0.061966	4.815368
307.347796	7999.975522	12.964544	-0.061939	4.815366
307.453685	8000.078810	12.969549	-0.061959	4.815395
307.341459	7999.954013	12.974554	-0.061938	4.815360
307.317119	8000.048728	12.979559	-0.061933	4.815387
307.403098	8000.009522	12.984563	-0.061949	4.815375
307.303020	7999.961887	12.989568	-0.061930	4.815362
307.322743	8000.004956	12.994573	-0.061934	4.815375
307.497997	7999.975782	12.999578	-0.061966	4.815365
307.475716	8000.006397	13.004583	-0.061962	4.815374
307.575863	7999.990942	13.009587	-0.061980	4.815369
307.488333	7999.958479	13.014592	-0.061964	4.815360
307.601620	8000.043719	13.019597	-0.061985	4.815385
307.654007	7999.968682	13.024602	-0.061994	4.815362
307.586888	7999.987865	13.029607	-0.061982	4.815368
307.495960	8000.013066	13.034611	-0.061965	4.815376
307.683261	8000.007607	13.039616	-0.061999	4.815374
307.590046	8000.057356	13.044621	-0.061982	4.815389
307.553589	7999.991535	13.049626	-0.061975	4.815370
307.374808	8000.049485	13.054631	-0.061941	4.815387
307.486995	8000.022471	13.059635	-0.061962	4.815379
307.419026	7999.977506	13.064640	-0.061949	4.815366
307.641419	8000.028212	13.069645	-0.061991	4.815380
307.684229	7999.994704	13.074650	-0.061998	4.815370
307.710128	8000.025049	13.079655	-0.062003	4.815379
307.638619	8000.025988	13.084659	-0.061990	4.815379
307.645499	8000.070983	13.089664	-0.061991	4.815392
307.609157	8000.061816	13.094669	-0.061984	4.815390
307.411492	8000.043560	13.099674	-0.061947	4.815385
307.602359	8000.052056	13.104679	-0.061982	4.815387
307.590392	8000.040086	13.109683	-0.061980	4.815384
307.438189	7999.989449	13.114688	-0.061951	4.815370
307.492010	8000.021326	13.119693	-0.061961	4.815379
307.519472	8000.023906	13.124698	-0.061966	4.815379
307.608232	7999.991159	13.129703	-0.061983	4.815369
307.528561	8000.033650	13.134707	-0.061968	4.815382
307.628323	8000.008568	13.139712	-0.061986	4.815374
307.753092	8000.032002	13.144717	-0.062009	4.815380
307.486959	7999.994440	13.149722	-0.061959	4.815371
307.676719	8000.005055	13.154727	-0.061995	4.815373
307.629891	7999.990370	13.159731	-0.061986	4.815369
307.621745	7999.979532	13.164736	-0.061984	4.815366
307.436583	7999.989276	13.169741	-0.061950	4.815370
307.606231	7999.937561	13.174746	-0.061981	4.815354
307.745277	8000.021090	13.179751	-0.062007	4.815377
307.551253	7999.980448	13.184755	-0.061970	4.815366
307.538107	7999.975941	13.189760	-0.061968	4.815365
307.679926	8000.038138	13.194765	-0.061994	4.815383
307.561484	7999.960269	13.199770	-0.061972	4.815360
307.578386	8000.008636	13.204775	-0.061975	4.815375
307.586785	7999.971351	13.209779	-0.061976	4.815364
307.563433	7999.985915	13.214784	-0.061972	4.815368
307.655497	8000.064389	13.219789	-0.061989	4.815390
307.518100	8000.072787	13.224794	-0.061963	4.815394
307.737791	8000.072141	13.229799	-0.062004	4.815392
307.573755	8000.011687	13.234803	-0.061973	4.815375
307.588418	8000.003365	13.239808	-0.061976	4.815373
307.596705	8000.035556	13.244813	-0.061977	4.815382
307.541824	8000.008979	13.249818	-0.061967	4.815375
307.550410	8000.015522	13.254823	-0.061968	4.815377
307.746875	8000.011284	13.259827	-0.062005	4.815375
307.876932	7999.983498	13.264832	-0.062029	4.815366
307.773707	8000.056597	13.269837	-0.062009	4.815388
307.871459	8000.074238	13.274842	-0.062027	4.815392
307.850645	8000.067466	13.279847	-0.062023	4.815390
307.786572	8000.039667	13.284851	-0.062011	4.815383
307.842904	8000.012797	13.289856	-0.062022	4.815375
307.997092	8000.096578	13.294861	-0.062050	4.815398
307.870341	8000.064533	13.299866	-0.062026	4.815390
307.595141	8000.072783	13.304871	-0.061975	4.815393
307.706654	7999.991244	13.309875	-0.061996	4.815369
307.840360	7999.968863	13.314880	-0.062020	4.815362
307.704538	8000.073488	13.319885	-0.061995	4.815393
307.749522	7999.942745	13.324890	-0.062003	4.815355
307.995646	8000.002396	13.329895	-0.062049	4.815371
307.990120	8000.058944	13.334899	-0.062048	4.815387
307.696518	8000.047648	13.339904	-0.061993	4.815385
307.728408	8000.020372	13.344909	-0.061999	4.815377
307.841620	7999.969859	13.349914	-0.062020	4.815362
307.694317	8000.039020	13.354919	-0.061992	4.815383
307.671455	8000.055730	13.359923	-0.061988	4.815388
307.837076	7999.986847	13.364928	-0.062018	4.815367
307.811097	7999.981058	13.369933	-0.062013	4.815365
307.568377	8000.005881	13.374938	-0.061968	4.815374
307.722206	8000.035141	13.379943	-0.061996	4.815382
307.699173	8000.056124	13.384947	-0.061992	4.815388
307.579802	8000.026339	13.389952	-0.061970	4.815380
307.880715	7999.993904	13.394957	-0.062025	4.815369
307.914955	7999.976287	13.399962	-0.062032	4.815364
307.868666	8000.047123	13.404967	-0.062023	4.815385
307.705985	8000.041205	13.409971	-0.061993	4.815384
307.607789	7999.972223	13.414976	-0.061974	4.815364
307.715043	7999.999642	13.419981	-0.061994	4.815371
307.506316	8000.013270	13.424986	-0.061955	4.815376
307.628375	8000.024901	13.429991	-0.061977	4.815379
307.760823	8000.002499	13.434995	-0.062002	4.815372
307.649607	7999.948265	13.440000	-0.061981	4.815357
307.974962	7999.983576	13.445005	-0.062042	4.815365
307.841333	7999.963175	13.450010	-0.062016	4.815360
307.727030	8000.027539	13.455015	-0.061995	4.815380
307.602315	8000.057525	13.460019	-0.061972	4.815389
307.750186	8000.000105	13.465024	-0.061999	4.815371
307.651294	8000.002727	13.470029	-0.061981	4.815373
307.678079	7999.981780	13.475034	-0.061985	4.815366
307.718730	8000.018784	13.480039	-0.061993	4.815377
307.782022	8000.046542	13.485043	-0.062004	4.815385
307.801679	8000.078922	13.490048	-0.062008	4.815394
307.724631	8000.045564	13.495053	-0.061993	4.815385
307.874747	7999.982837	13.500058	-0.062021	4.815366
307.905881	8000.014338	13.505063	-0.062027	4.815375
307.841988	8000.002576	13.510067	-0.062015	4.815372
308.013537	7999.976547	13.515072	-0.062047	4.815363
307.882206	8000.070558	13.520077	-0.062022	4.815391
307.678119	8000.008370	13.525082	-0.061984	4.815374
307.799605	8000.018923	13.530087	-0.062006	4.815377
307.737374	8000.048876	13.535091	-0.061995	4.815386
307.680921	7999.999826	13.540096	-0.061984	4.815372
307.826696	8000.047124	13.545101	-0.062011	4.815385
307.947797	8000.010638	13.550106	-0.062033	4.815374
307.884799	8000.095093	13.555111	-0.062022	4.815399
307.768014	8000.037559	13.560115	-0.062000	4.815382
307.812041	8000.053241	13.565120	-0.062008	4.815387
308.021414	8000.073803	13.570125	-0.062047	4.815392
307.793634	7999.984499	13.575130	-0.062004	4.815367
307.777363	7999.982078	13.580135	-0.062001	4.815366
307.759976	7999.991397	13.585139	-0.061997	4.815369
307.720181	7999.988586	13.590144	-0.061990	4.815368
307.687582	8000.055373	13.595149	-0.061984	4.815388
307.728749	7999.989770	13.600154	-0.061991	4.815369
307.857833	7999.963037	13.605159	-0.062015	4.815360
307.806009	7999.938648	13.610163	-0.062005	4.815353
307.744040	8000.043429	13.615168	-0.061994	4.815384
307.775084	8000.078136	13.620173	-0.061999	4.815394
307.599551	8000.023904	13.625178	-0.061966	4.815379
307.745281	8000.016687	13.630183	-0.061993	4.815376
307.915079	8000.034454	13.635187	-0.062025	4.815381
307.900368	8000.012819	13.640192	-0.062022	4.815375
307.692722	7999.986915	13.645197	-0.061983	4.815368
307.759072	7999.986933	13.650202	-0.061995	4.815368
307.910928	8000.033263	13.655207	-0.062023	4.815380
307.765646	8000.026565	13.660211	-0.061996	4.815379
307.767551	8000.032997	13.665216	-0.061996	4.815381
307.706215	8000.054414	13.670221	-0.061985	4.815388
307.635529	7999.969854	13.675226	-0.061971	4.815363
307.598682	8000.052604	13.680231	-0.061965	4.815388
307.746991	8000.072152	13.685235	-0.061992	4.815393
307.712165	8000.019185	13.690240	-0.061985	4.815377
307.714393	8000.068379	13.695245	-0.061986	4.815392
307.648337	8000.038409	13.700250	-0.061973	4.815383
307.859184	8000.049375	13.705255	-0.062012	4.815385
307.845005	8000.010646	13.710259	-0.062009	4.815374
307.566332	7999.970738	13.715264	-0.061957	4.815364
307.677393	8000.011046	13.720269	-0.061978	4.815375
307.585267	7999.966750	13.725274	-0.061961	4.815363
307.569939	8000.016721	13.730279	-0.061958	4.815377
307.746282	8000.028182	13.735283	-0.061990	4.815380
307.933384	7999.937208	13.740288	-0.062025	4.815352
307.809864	8000.052726	13.745293	-0.062002	4.815387
307.825100	7999.978142	13.750298	-0.062005	4.815365
307.834243	7999.975074	13.755303	-0.062006	4.815364
307.797801	7999.994765	13.760307	-0.061999	4.815370
307.778210	8000.027563	13.765312	-0.061995	4.815380
307.900042	8000.096912	13.770317	-0.062018	4.815399
307.723248	8000.028763	13.775322	-0.061985	4.815380
307.726265	8000.039489	13.780327	-0.061985	4.815383
307.956046	8000.030459	13.785331	-0.062028	4.815380
307.901000	7999.998534	13.790336	-0.062017	4.815370
307.947354	8000.052735	13.795341	-0.062026	4.815386
307.772652	8000.038067	13.800346	-0.061993	4.815383
307.670998	8000.006439	13.805351	-0.061974	4.815374
307.686807	8000.060133	13.810355	-0.061977	4.815390
307.799638	7999.991443	13.815360	-0.061998	4.815369
307.970771	8000.009232	13.820365	-0.062030	4.815373
307.762238	7999.967280	13.825370	-0.061991	4.815362
307.882434	8000.017361	13.830375	-0.062013	4.815376
307.953754	8000.049528	13.835379	-0.062026	4.815385
307.748738	7999.975568	13.840384	-0.061988	4.815365
307.796403	8000.037272	13.845389	-0.061996	4.815382
307.718741	8000.029558	13.850394	-0.061982	4.815380
307.985370	8000.031828	13.855399	-0.062031	4.815380
307.934515	8000.127174	13.860403	-0.062022	4.815408
307.723426	8000.044560	13.865408	-0.061982	4.815385
307.955965	8000.078333	13.870413	-0.062025	4.815394
307.910746	8000.000608	13.875418	-0.062017	4.815371
307.891897	8000.038763	13.880423	-0.062013	4.815382
307.928854	8000.015846	13.885427	-0.062020	4.815375
307.890839	7999.983135	13.890432	-0.062013	4.815366
307.864651	8000.022237	13.895437	-0.062008	4.815378
307.855229	7999.994276	13.900442	-0.062006	4.815370
307.937675	8000.103590	13.905447	-0.062021	4.815401
307.822279	8000.076009	13.910451	-0.061999	4.815394
307.790862	8000.029512	13.915456	-0.061993	4.815380
307.859050	8000.043456	13.920461	-0.062006	4.815384
308.063322	7999.949560	13.925466	-0.062044	4.815355
307.964221	8000.034485	13.930471	-0.062025	4.815381
307.959937	8000.072881	13.935475	-0.062024	4.815392
307.838152	8000.036643	13.940480	-0.062001	4.815382
307.859867	8000.124641	13.945485	-0.062005	4.815408
307.812702	8000.063986	13.950490	-0.061996	4.815390
307.898483	8000.051499	13.955495	-0.062012	4.815386
308.025456	8000.051454	13.960499	-0.062036	4.815385
307.840571	7999.974620	13.965504	-0.062001	4.815364
308.171239	8000.070948	13.970509	-0.062062	4.815390
307.947969	8000.010579	13.975514	-0.062021	4.815374
307.895887	8000.119800	13.980519	-0.062011	4.815406
307.691350	8000.066156	13.985523	-0.061973	4.815391
307.823226	7999.997782	13.990528	-0.061997	4.815371
307.982171	8000.077366	13.995533	-0.062027	4.815393
307.847789	7999.994956	14.000538	-0.062001	4.815370
308.102884	8000.051550	14.005543	-0.062049	4.815385
308.170401	8000.099688	14.010547	-0.062061	4.815399
308.012248	8000.050020	14.015552	-0.062032	4.815385
307.897283	8000.116510	14.020557	-0.062010	4.815405
307.878920	8000.045644	14.025562	-0.062006	4.815385
307.907135	8000.102751	14.030567	-0.062012	4.815401
307.826584	8000.067197	14.035571	-0.061996	4.815391
307.881149	8000.006092	14.040576	-0.062006	4.815373
308.047609	8000.101834	14.045581	-0.062037	4.815400
307.876761	8000.063714	14.050586	-0.062005	4.815390
307.859323	8000.065549	14.055591	-0.062002	4.815390
308.134742	8000.108584	14.060595	-0.062053	4.815402
307.987259	8000.049472	14.065600	-0.062025	4.815385
307.812250	8000.070073	14.070605	-0.061993	4.815392
307.824908	8000.043547	14.075610	-0.061995	4.815384
307.783697	8000.025748	14.080615	-0.061987	4.815379
307.789544	8000.051485	14.085619	-0.061988	4.815387
307.858776	8000.014139	14.090624	-0.062001	4.815375
308.108863	8000.086684	14.095629	-0.062047	4.815395
308.096828	8000.056541	14.100634	-0.062045	4.815387
308.110350	8000.089888	14.105639	-0.062047	4.815396
308.187699	8000.113605	14.110643	-0.062061	4.815403
307.913244	8000.051319	14.115648	-0.062010	4.815386
308.116345	8000.074983	14.120653	-0.062048	4.815392
308.159675	8000.102411	14.125658	-0.062056	4.815400
307.980191	8000.144316	14.130663	-0.062022	4.815413
308.036167	8000.114232	14.135667	-0.062032	4.815404
308.042148	8000.094009	14.140672	-0.062033	4.815398
307.997173	8000.133868	14.145677	-0.062025	4.815410
307.850408	7999.996738	14.150682	-0.061997	4.815370
307.971917	8000.030807	14.155687	-0.062020	4.815380
307.959119	8000.046615	14.160691	-0.062017	4.815385
307.797074	8000.001159	14.165696	-0.061987	4.815372
307.910200	8000.057535	14.170701	-0.062008	4.815388
307.772788	8000.040279	14.175706	-0.061982	4.815384
307.958659	8000.061519	14.180711	-0.062017	4.815389
307.863674	8000.130479	14.185715	-0.061999	4.815409
307.920054	8000.082231	14.190720	-0.062009	4.815395
308.000214	8000.096374	14.195725	-0.062024	4.815399
307.891468	8000.069972	14.200730	-0.062004	4.815392
307.854389	8000.031932	14.205735	-0.061996	4.815381
308.011114	7999.974659	14.210739	-0.062025	4.815363
307.949231	7999.980033	14.215744	-0.062014	4.815365
307.922564	8000.066159	14.220749	-0.062009	4.815390
307.843836	8000.078736	14.225754	-0.061994	4.815395
307.964454	8000.105308	14.230759	-0.062016	4.815402
307.877302	8000.144468	14.235763	-0.062000	4.815414
307.846331	8000.015672	14.240768	-0.061994	4.815376
308.024395	8000.029300	14.245773	-0.062027	4.815379
307.696532	8000.023850	14.250778	-0.061966	4.815379
307.936593	8000.056678	14.255783	-0.062010	4.815388
308.107008	8000.107592	14.260787	-0.062042	4.815402
307.823687	8000.025919	14.265792	-0.061989	4.815379
307.887970	7999.134457	14.270797	-0.062000	4.815119
307.906314	7995.971254	14.275802	-0.062001	4.814194
307.918223	7990.567117	14.280807	-0.062000	4.812615
307.861196	7983.862937	14.285811	-0.061985	4.810656
307.609356	7976.590536	14.290816	-0.061933	4.808530
307.660704	7968.975240	14.295821	-0.061937	4.806302
307.580743	7961.181192	14.300826	-0.061917	4.804021
307.532972	7953.329561	14.305831	-0.061903	4.801722
307.562246	7945.336941	14.310835	-0.061903	4.799381
307.647546	7937.444898	14.315840	-0.061914	4.797067
307.653390	7929.379847	14.320845	-0.061910	4.794702
307.496475	7921.401496	14.325850	-0.061875	4.792361
307.616338	7913.342870	14.330855	-0.061892	4.789995
307.555303	7905.418445	14.335859	-0.061875	4.787668
307.386562	7897.308376	14.340864	-0.061838	4.785286
307.474762	7889.493706	14.345869	-0.061850	4.782988
307.366345	7881.348988	14.350874	-0.061824	4.780593
307.177147	7873.409890	14.355879	-0.061783	4.778257
307.205753	7865.368466	14.360883	-0.061783	4.775889
307.081778	7857.357633	14.365888	-0.061755	4.773530
307.318241	7849.398899	14.370893	-0.061794	4.771184
307.124316	7841.350659	14.375898	-0.061752	4.768811
307.367189	7833.401917	14.380903	-0.061792	4.766465
307.250849	7825.410268	14.385907	-0.061765	4.764107
307.085244	7817.414632	14.390912	-0.061729	4.761746
307.167275	7809.348877	14.395917	-0.061739	4.759363
307.177642	7801.361264	14.400922	-0.061735	4.757002
307.149486	7793.309634	14.405927	-0.061724	4.754621
307.023146	7785.308406	14.410931	-0.061696	4.752254
306.967963	7777.268792	14.415936	-0.061680	4.749874
306.969274	7769.308677	14.420941	-0.061675	4.747516
306.879776	7761.290455	14.425946	-0.061653	4.745140
307.096885	7753.344814	14.430951	-0.061688	4.742784
306.920248	7745.342127	14.435955	-0.061650	4.740410
306.912177	7737.330525	14.440960	-0.061643	4.738033
307.119121	7729.325113	14.445965	-0.061676	4.735655
306.952310	7721.314722	14.450970	-0.061640	4.733276
306.851517	7713.304868	14.455975	-0.061615	4.730895
306.834701	7705.343968	14.460979	-0.061607	4.728528
306.733779	7697.281389	14.465984	-0.061583	4.726129
306.646395	7689.310099	14.470989	-0.061561	4.723756
306.457399	7681.275934	14.475994	-0.061521	4.721364
306.553861	7673.331144	14.480999	-0.061533	4.718996
306.553748	7665.373791	14.486003	-0.061528	4.716624
306.509581	7657.308125	14.491008	-0.061514	4.714218
306.697293	7649.280898	14.496013	-0.061544	4.711822
306.560566	7641.245723	14.501018	-0.061513	4.709423
306.519405	7633.271856	14.506023	-0.061500	4.707041
306.423498	7625.280755	14.511027	-0.061477	4.704652
306.598877	7617.311397	14.516032	-0.061504	4.702269
306.571488	7609.310153	14.521037	-0.061494	4.699875
306.342196	7601.336630	14.526042	-0.061445	4.697488
306.406662	7593.274403	14.531047	-0.061452	4.695073
306.330404	7585.320585	14.536051	-0.061433	4.692690
306.081161	7577.193816	14.541056	-0.061381	4.690254
306.092949	7569.301886	14.546061	-0.061378	4.687887
306.221135	7561.237847	14.551066	-0.061396	4.685466
306.162883	7553.311984	14.556071	-0.061380	4.683086
306.050583	7545.303653	14.561075	-0.061354	4.680680
306.018087	7537.264617	14.566080	-0.061342	4.678264
306.052658	7529.277842	14.571085	-0.061343	4.675862
305.891355	7521.175942	14.576090	-0.061308	4.673424
305.958018	7513.152003	14.581095	-0.061315	4.671008
305.861281	7505.218487	14.586099	-0.061291	4.668619
305.676527	7497.192375	14.591104	-0.061252	4.666200
305.887531	7489.246700	14.596109	-0.061286	4.663804
305.974133	7481.267291	14.601114	-0.061296	4.661397
305.876215	7473.221993	14.606119	-0.061273	4.658968
305.662912	7465.261130	14.611123	-0.061228	4.656564
305.432013	7457.192848	14.616128	-0.061179	4.654127
305.498416	7449.183542	14.621133	-0.061186	4.651705
305.437863	7441.173874	14.626138	-0.061170	4.649283
305.519706	7433.214200	14.631143	-0.061180	4.646874
305.647920	7425.194843	14.636147	-0.061198	4.644445
305.567143	7417.229607	14.641152	-0.061178	4.642032
305.538767	7409.188354	14.646157	-0.061167	4.639595
305.458058	7401.249009	14.651162	-0.061147	4.637187
305.481684	7393.178243	14.656167	-0.061146	4.634739
305.410362	7385.198970	14.661171	-0.061127	4.632316
305.471810	7377.130599	14.666176	-0.061133	4.629865
305.597508	7369.223702	14.671181	-0.061151	4.627462
305.343758	7361.134658	14.676186	-0.061099	4.625003
305.246040	7353.219445	14.681191	-0.061075	4.622595
305.389354	7345.212191	14.686195	-0.061096	4.620158
305.262334	7337.195649	14.691200	-0.061067	4.617716
305.087246	7329.177242	14.696205	-0.061029	4.615273
304.868183	7321.147796	14.701210	-0.060983	4.612825
305.037521	7313.115523	14.706215	-0.061009	4.610375
305.112733	7305.186686	14.711219	-0.061018	4.607955
304.869171	7297.121079	14.716224	-0.060967	4.605492
304.938685	7289.188411	14.721229	-0.060975	4.603068
304.575959	7281.141819	14.726234	-0.060902	4.600609
304.754315	7273.182808	14.731239	-0.060930	4.598174
304.900503	7265.162714	14.736243	-0.060952	4.595720
304.778267	7257.111556	14.741248	-0.060924	4.593255
304.725609	7249.099305	14.746253	-0.060908	4.590800
304.739933	7241.096340	14.751258	-0.060906	4.588347
304.617332	7233.089788	14.756263	-0.060877	4.585892
304.810151	7225.137752	14.761267	-0.060908	4.583452
304.745022	7217.103064	14.766272	-0.060891	4.580985
304.889910	7209.184988	14.771277	-0.060912	4.578553
304.671911	7201.173562	14.776282	-0.060866	4.576091
304.552208	7193.162191	14.781287	-0.060839	4.573628
304.432298	7185.090267	14.786291	-0.060811	4.571144
304.373469	7177.051985	14.791296	-0.060794	4.568669
304.348402	7169.068638	14.796301	-0.060784	4.566211
304.244558	7161.107122	14.801306	-0.060760	4.563757
304.233555	7153.117178	14.806311	-0.060752	4.561293
304.232275	7145.126466	14.811315	-0.060747	4.558828
303.953416	7137.145328	14.816320	-0.060690	4.556364
304.164262	7129.140140	14.821325	-0.060723	4.553892
304.025939	7120.999458	14.826330	-0.060692	4.551377
304.089906	7113.087470	14.831335	-0.060699	4.548931
304.125832	7105.110245	14.836339	-0.060700	4.546463
304.043992	7097.089563	14.841344	-0.060680	4.543980
304.065397	7089.137244	14.846349	-0.060678	4.541518
304.137308	7081.066059	14.851354	-0.060686	4.539017
304.183928	7073.110196	14.856359	-0.060690	4.536551
304.151318	7065.110830	14.861363	-0.060678	4.534069
304.045826	7057.111293	14.866368	-0.060653	4.531586
304.139701	7049.089777	14.871373	-0.060665	4.529096
303.887352	7041.086999	14.876378	-0.060613	4.526609
303.895731	7033.038753	14.881383	-0.060609	4.524107
303.868794	7025.162788	14.886387	-0.060599	4.521657
303.628143	7017.111129	14.891392	-0.060548	4.519150
303.779573	7009.150340	14.896397	-0.060571	4.516672
303.610509	7001.080103	14.901402	-0.060534	4.514157
303.636016	6993.055973	14.906407	-0.060534	4.511656
303.621826	6985.063626	14.911411	-0.060526	4.509163
303.569901	6977.044019	14.916416	-0.060511	4.506660
303.467353	6969.071301	14.921421	-0.060486	4.504170
303.475117	6961.064133	14.926426	-0.060482	4.501668
303.585480	6953.032565	14.931431	-0.060498	4.499158
303.639310	6945.089774	14.936435	-0.060502	4.496674
303.604097	6937.033494	14.941440	-0.060490	4.494153
303.425466	6929.046891	14.946445	-0.060452	4.491651
303.079634	6921.008633	14.951450	-0.060382	4.489132
303.206201	6913.048089	14.956455	-0.060400	4.486637
303.228831	6905.060128	14.961459	-0.060399	4.484131
303.171238	6897.080427	14.966464	-0.060383	4.481627
303.414157	6889.043473	14.971469	-0.060423	4.479104
303.167279	6881.056839	14.976474	-0.060371	4.476594
303.191197	6873.030191	14.981479	-0.060371	4.474071
303.312915	6865.032803	14.986483	-0.060388	4.471556
303.083510	6856.979310	14.991488	-0.060340	4.469020
302.958387	6849.019504	14.996493	-0.060311	4.466513
303.143031	6841.037884	15.001498	-0.060340	4.463999
303.213383	6833.030350	15.006503	-0.060348	4.461475
302.969492	6825.073605	15.011507	-0.060297	4.458964
302.788114	6816.996090	15.016512	-0.060258	4.456414
302.895678	6809.053163	15.021517	-0.060273	4.453906
302.905315	6800.959825	15.026522	-0.060269	4.451349
302.773584	6793.009166	15.031527	-0.060239	4.448835
302.694642	6785.014038	15.036531	-0.060219	4.446305
302.757446	6776.999958	15.041536	-0.060225	4.443769
302.716905	6768.998702	15.046541	-0.060212	4.441235
302.749361	6761.070006	15.051546	-0.060213	4.438723
302.605872	6752.990685	15.056551	-0.060181	4.436160
302.529791	6744.993873	15.061555	-0.060162	4.433623
302.311148	6736.926980	15.066560	-0.060115	4.431062
302.527350	6728.993301	15.071565	-0.060150	4.428543
302.409869	6720.960827	15.076570	-0.060123	4.425990
302.560445	6712.982137	15.081575	-0.060146	4.423453
302.456266	6705.003889	15.086579	-0.060121	4.420914
302.455821	6696.976758	15.091584	-0.060116	4.418359
302.281426	6688.954958	15.096589	-0.060078	4.415803
302.169529	6680.966299	15.101594	-0.060052	4.413256
302.170031	6672.930641	15.106599	-0.060046	4.410694
302.214382	6665.001676	15.111603	-0.060049	4.408164
302.066113	6656.940529	15.116608	-0.060016	4.405590
302.361780	6649.012805	15.121613	-0.060066	4.403059
302.282789	6640.926720	15.126618	-0.060046	4.400474
302.092446	6633.022925	15.131623	-0.060005	4.397945
302.220622	6624.977015	15.136627	-0.060024	4.395371
302.216182	6616.945816	15.141632	-0.060017	4.392799
302.030851	6608.949700	15.146637	-0.059977	4.390236
301.984345	6600.968591	15.151642	-0.059963	4.387678
301.922039	6592.936006	15.156647	-0.059946	4.385101
302.028662	6585.007296	15.161651	-0.059961	4.382557
301.956437	6576.971670	15.166656	-0.059942	4.379976
302.000733	6569.013504	15.171661	-0.059945	4.377419
301.927187	6560.966027	15.176666	-0.059926	4.374831
302.010635	6552.967020	15.181671	-0.059936	4.372258
301.849517	6544.939443	15.186675	-0.059901	4.369673
301.666409	6536.974275	15.191680	-0.059861	4.367106
301.897359	6528.996305	15.196685	-0.059899	4.364537
301.629752	6520.988982	15.201690	-0.059844	4.361953
301.641719	6513.015912	15.206695	-0.059841	4.359380
301.727022	6505.085748	15.211699	-0.059851	4.356821
301.494552	6496.942368	15.216704	-0.059803	4.354189
301.281454	6488.877975	15.221709	-0.059757	4.351580
301.433567	6480.834292	15.226714	-0.059780	4.348980
301.337132	6472.889162	15.231719	-0.059757	4.346408
301.211103	6464.956138	15.236723	-0.059728	4.343838
301.246357	6456.916630	15.241728	-0.059729	4.341233
301.346551	6448.946041	15.246733	-0.059743	4.338650
301.234056	6440.941376	15.251738	-0.059716	4.336052
301.279663	6432.922798	15.256743	-0.059720	4.333450
301.175271	6424.945895	15.261747	-0.059695	4.330858
300.962723	6416.933912	15.266752	-0.059650	4.328253
301.040631	6408.923353	15.271757	-0.059659	4.325649
300.938952	6400.964735	15.276762	-0.059635	4.323058
300.912025	6392.928742	15.281767	-0.059624	4.320442
300.839094	6384.997351	15.286771	-0.059605	4.317857
301.015152	6376.946364	15.291776	-0.059633	4.315234
301.061712	6368.917530	15.296781	-0.059636	4.312616
300.927341	6360.897742	15.301786	-0.059606	4.309997
300.672680	6352.934435	15.306791	-0.059553	4.307395
300.733436	6344.914198	15.311795	-0.059559	4.304775
300.752678	6336.928447	15.316800	-0.059557	4.302164
300.876764	6328.935502	15.321805	-0.059575	4.299550
300.709050	6320.936287	15.326810	-0.059538	4.296930
300.582683	6312.920061	15.331815	-0.059509	4.294303
300.771966	6304.870607	15.336819	-0.059539	4.291666
300.631446	6296.871277	15.341824	-0.059508	4.289041
300.631089	6288.901006	15.346829	-0.059502	4.286426
300.464561	6280.944521	15.351834	-0.059466	4.283812
300.494913	6272.950955	15.356839	-0.059466	4.281185
300.527524	6264.940398	15.361843	-0.059467	4.278552
300.347914	6256.904156	15.366848	-0.059428	4.275907
300.391531	6248.892803	15.371853	-0.059431	4.273270
300.253827	6240.867414	15.376858	-0.059400	4.270625
300.241724	6232.855131	15.381863	-0.059392	4.267984
300.150702	6224.860315	15.386867	-0.059370	4.265347
299.999118	6216.923170	15.391872	-0.059336	4.262726
300.112813	6208.890296	15.396877	-0.059352	4.260075
299.952326	6200.936849	15.401882	-0.059317	4.257445
299.876717	6192.842595	15.406887	-0.059297	4.254769
299.995135	6184.927409	15.411891	-0.059314	4.252151
299.837946	6176.870031	15.416896	-0.059279	4.249482
299.799079	6168.914378	15.421901	-0.059267	4.246847
299.767425	6160.896630	15.426906	-0.059256	4.244189
299.803259	6152.915903	15.431911	-0.059257	4.241543
299.688031	6144.905873	15.436915	-0.059230	4.238883
299.552470	6136.926880	15.441920	-0.059200	4.236232
299.835606	6128.904287	15.446925	-0.059247	4.233569
299.660420	6120.868912	15.451930	-0.059209	4.230896
299.850658	6112.890909	15.456935	-0.059239	4.228243
299.835102	6104.899499	15.461939	-0.059231	4.225583
299.510205	6096.942873	15.466944	-0.059165	4.222929
299.431457	6088.952245	15.471949	-0.059145	4.220265
299.619289	6080.920373	15.476954	-0.059174	4.217588
299.677723	6072.889942	15.481959	-0.059180	4.214908
299.509752	6064.956499	15.486963	-0.059143	4.212257
299.405202	6056.912254	15.491968	-0.059118	4.209568
299.361162	6048.960012	15.496973	-0.059105	4.206908
299.338576	6040.881580	15.501978	-0.059095	4.204205
299.255097	6032.954733	15.506983	-0.059074	4.201550
299.444299	6024.965732	15.511987	-0.059104	4.198875
299.277244	6016.942679	15.516992	-0.059068	4.196184
299.421909	6008.856379	15.521997	-0.059089	4.193472
299.241431	6000.806058	15.527002	-0.059050	4.190768
299.328397	5992.857447	15.532007	-0.059061	4.188099
299.066585	5984.863825	15.537011	-0.059007	4.185410
298.957060	5976.908567	15.542016	-0.058981	4.182733
299.204839	5968.875401	15.547021	-0.059022	4.180032
298.790547	5960.943183	15.552026	-0.058940	4.177356
298.696439	5952.887117	15.557031	-0.058917	4.174640
298.835956	5944.909111	15.562035	-0.058937	4.171952
298.874048	5936.874837	15.567040	-0.058939	4.169241
298.781541	5928.900079	15.572045	-0.058917	4.166547
298.742712	5920.896380	15.577050	-0.058904	4.163843
298.577438	5912.948355	15.582055	-0.058868	4.161154
298.607161	5904.947223	15.587059	-0.058868	4.158447
298.843893	5896.881495	15.592064	-0.058907	4.155720
298.878774	5888.888752	15.597069	-0.058908	4.153013
298.708414	5880.874274	15.602074	-0.058871	4.150294
298.447617	5872.860003	15.607079	-0.058817	4.147572
298.750121	5864.872705	15.612083	-0.058868	4.144865
298.810592	5856.881596	15.617088	-0.058874	4.142152
298.569460	5848.899985	15.622093	-0.058823	4.139436
298.379320	5840.900791	15.627098	-0.058783	4.136714
298.342879	5832.895930	15.632103	-0.058771	4.133989
298.444310	5824.871233	15.637107	-0.058784	4.131258
298.319419	5816.860018	15.642112	-0.058755	4.128526
298.387710	5808.872748	15.647117	-0.058763	4.125803
298.419884	5800.912177	15.652122	-0.058763	4.123088
298.160443	5792.869787	15.657127	-0.058710	4.120338
298.153414	5784.942278	15.662131	-0.058703	4.117630
298.095276	5776.908705	15.667136	-0.058687	4.114882
298.115258	5768.891288	15.672141	-0.058685	4.112140
297.984701	5760.844773	15.677146	-0.058656	4.109383
297.903113	5752.849240	15.682151	-0.058635	4.106643
297.800386	5744.868081	15.687155	-0.058610	4.103906
297.733062	5736.861832	15.692160	-0.058593	4.101158
297.745669	5728.907919	15.697165	-0.058590	4.098428
298.106262	5720.858653	15.702170	-0.058651	4.095668
297.964693	5712.866839	15.707175	-0.058620	4.092919
297.866919	5704.877845	15.712179	-0.058596	4.090170
297.947351	5696.887289	15.717184	-0.058606	4.087421
297.888319	5688.892171	15.722189	-0.058589	4.084666
297.894749	5680.951502	15.727194	-0.058585	4.081929
297.884769	5672.916371	15.732199	-0.058578	4.079158
297.872622	5664.969090	15.737203	-0.058570	4.076415
297.611975	5656.897077	15.742208	-0.058516	4.073623
297.743611	5648.895260	15.747213	-0.058536	4.070860
297.721278	5640.924023	15.752218	-0.058526	4.068103
297.416562	5632.867800	15.757223	-0.058464	4.065311
297.449171	5624.962957	15.762227	-0.058465	4.062573
297.496040	5616.890835	15.767232	-0.058468	4.059777
297.558440	5608.962217	15.772237	-0.058474	4.057028
297.622036	5600.916592	15.777242	-0.058481	4.054237
297.508585	5592.915327	15.782247	-0.058454	4.051457
297.592239	5584.924823	15.787251	-0.058465	4.048681
297.256891	5576.930479	15.792256	-0.058397	4.045897
297.473090	5568.952552	15.797261	-0.058432	4.043124
297.387549	5560.926506	15.802266	-0.058410	4.040328
297.313721	5552.952132	15.807271	-0.058391	4.037548
297.144380	5544.930997	15.812275	-0.058354	4.034748
297.162052	5536.809967	15.817280	-0.058352	4.031915
297.174017	5528.845045	15.822285	-0.058349	4.029134
297.155180	5520.885177	15.827290	-0.058340	4.026352
297.276929	5512.901486	15.832295	-0.058358	4.023562
297.369722	5504.867475	15.837299	-0.058369	4.020752
297.226147	5496.894909	15.842304	-0.058337	4.017958
297.161352	5488.899535	15.847309	-0.058320	4.015156
297.230209	5480.937664	15.852314	-0.058327	4.012365
297.166790	5472.878702	15.857319	-0.058310	4.009536
297.204430	5464.965807	15.862323	-0.058312	4.006758
297.088886	5456.881432	15.867328	-0.058285	4.003916
297.044828	5448.934530	15.872333	-0.058271	4.001121
296.916833	5440.942026	15.877338	-0.058242	3.998306
296.828057	5432.911769	15.882343	-0.058220	3.995477
297.129541	5424.894185	15.887347	-0.058271	3.992657
296.847907	5416.867347	15.892352	-0.058213	3.989821
296.807825	5408.899754	15.897357	-0.058200	3.987009
296.907402	5400.880961	15.902362	-0.058214	3.984179
296.730779	5392.904528	15.907367	-0.058175	3.981357
296.830746	5384.946500	15.912371	-0.058189	3.978545
296.719229	5376.931673	15.917376	-0.058163	3.975707
296.874974	5368.905627	15.922381	-0.058186	3.972867
296.654377	5360.888093	15.927386	-0.058140	3.970022
296.543194	5352.912570	15.932391	-0.058114	3.967191
296.772344	5344.939751	15.937395	-0.058151	3.964366
296.599495	5336.947842	15.942400	-0.058113	3.961524
296.539603	5328.988805	15.947405	-0.058097	3.958694
296.545618	5320.979662	15.952410	-0.058093	3.955846
296.471020	5312.910931	15.957415	-0.058073	3.952973
296.479262	5304.916797	15.962419	-0.058070	3.950125
296.424768	5296.934999	15.967424	-0.058054	3.947279
296.545081	5288.957413	15.972429	-0.058071	3.944436
296.268009	5280.997236	15.977434	-0.058014	3.941590
296.169049	5273.017528	15.982439	-0.057990	3.938737
296.462915	5264.983122	15.987443	-0.058040	3.935870
296.237429	5256.992541	15.992448	-0.057992	3.933008
296.124527	5248.954305	15.997453	-0.057966	3.930128
296.112158	5240.995366	16.002458	-0.057958	3.927276
296.200928	5232.957911	16.007463	-0.057970	3.924396
295.983912	5225.040087	16.012467	-0.057924	3.921552
295.889343	5216.981080	16.017472	-0.057901	3.918656
296.066738	5209.004540	16.022477	-0.057928	3.915793
296.067395	5200.976849	16.027482	-0.057923	3.912907
295.904920	5192.940052	16.032487	-0.057888	3.910012
296.189436	5184.979832	16.037491	-0.057935	3.907150
296.057246	5176.950771	16.042496	-0.057905	3.904255
296.035480	5168.989492	16.047501	-0.057896	3.901383
295.972614	5161.012022	16.052506	-0.057879	3.898503
295.794390	5152.998995	16.057511	-0.057840	3.895605
295.612847	5144.983554	16.062515	-0.057801	3.892704
295.581597	5136.932600	16.067520	-0.057790	3.889792
295.713546	5129.021311	16.072525	-0.057809	3.886930
295.606187	5120.978610	16.077530	-0.057784	3.884015
295.575945	5112.999010	16.082535	-0.057773	3.881121
295.697805	5105.028426	16.087539	-0.057790	3.878232
295.700908	5097.005646	16.092544	-0.057785	3.875319
295.566963	5088.811627	16.097549	-0.057755	3.872339
295.255266	5080.841287	16.102554	-0.057691	3.869435
295.221009	5072.893744	16.107559	-0.057680	3.866542
295.287786	5064.934670	16.112563	-0.057687	3.863644
295.180080	5056.931141	16.117568	-0.057661	3.860725
295.191225	5048.975971	16.122573	-0.057658	3.857824
295.102948	5040.998060	16.127578	-0.057636	3.854910
294.987229	5032.963665	16.132583	-0.057609	3.851973
295.256705	5024.973861	16.137587	-0.057654	3.849058
295.182511	5016.984381	16.142592	-0.057635	3.846133
295.109754	5008.995822	16.147597	-0.057616	3.843207
295.007889	5001.030347	16.152602	-0.057592	3.840287
294.996868	4993.023322	16.157607	-0.057584	3.837350
295.181486	4985.019056	16.162611	-0.057613	3.834417
294.968416	4976.999161	16.167616	-0.057568	3.831467
294.985105	4968.979286	16.172621	-0.057566	3.828520
294.954512	4961.017493	16.177626	-0.057555	3.825591
294.861054	4953.052695	16.182631	-0.057532	3.822657
294.885722	4945.066102	16.187635	-0.057532	3.819716
294.947242	4937.059833	16.192640	-0.057538	3.816765
294.969209	4929.066249	16.197645	-0.057536	3.813817
294.828884	4921.056131	16.202650	-0.057505	3.810856
294.812395	4913.046795	16.207655	-0.057496	3.807896
294.794427	4905.085981	16.212659	-0.057488	3.804952
294.753758	4897.098943	16.217664	-0.057475	3.801995
294.926177	4889.084566	16.222669	-0.057502	3.799030
294.638443	4881.094225	16.227674	-0.057443	3.796062
294.674856	4873.082693	16.232679	-0.057444	3.793091
294.716071	4865.039318	16.237683	-0.057446	3.790106
294.538647	4857.044675	16.242688	-0.057408	3.787131
294.498401	4849.056601	16.247693	-0.057395	3.784160
294.398297	4841.074216	16.252698	-0.057371	3.781187
294.585777	4833.068313	16.257703	-0.057401	3.778210
294.395768	4825.106469	16.262707	-0.057360	3.775238
294.103799	4817.091055	16.267712	-0.057300	3.772242
294.197868	4809.103869	16.272717	-0.057312	3.769262
294.109127	4801.086478	16.277722	-0.057290	3.766264
294.242071	4793.092863	16.282727	-0.057310	3.763279
294.088220	4785.114764	16.287731	-0.057276	3.760290
293.965902	4777.131979	16.292736	-0.057248	3.757297
293.835610	4769.144449	16.297741	-0.057218	3.754300
293.670022	4761.098985	16.302746	-0.057182	3.751279
293.645823	4753.084566	16.307751	-0.057172	3.748269
293.767004	4745.075864	16.312755	-0.057189	3.745263
293.562304	4737.089731	16.317760	-0.057146	3.742255
293.521307	4729.106502	16.322765	-0.057133	3.739250
293.609957	4721.125718	16.327770	-0.057144	3.736246
293.613494	4713.113627	16.332775	-0.057139	3.733227
293.598944	4705.104204	16.337779	-0.057131	3.730205
293.558264	4697.120299	16.342784	-0.057118	3.727189
293.593606	4689.123179	16.347789	-0.057119	3.724169
293.488247	4681.197628	16.352794	-0.057095	3.721169
293.529207	4673.144650	16.357799	-0.057097	3.718122
293.757360	4665.142281	16.362803	-0.057134	3.715097
293.579191	4657.090977	16.367808	-0.057095	3.712040
293.565857	4649.071123	16.372813	-0.057087	3.708997
293.556377	4641.095420	16.377818	-0.057080	3.705969
293.053812	4633.173860	16.382823	-0.056981	3.702946
293.268269	4625.162258	16.387827	-0.057016	3.699904
293.176874	4617.191887	16.392832	-0.056994	3.696868
293.229397	4609.181002	16.397837	-0.056998	3.693817
293.270491	4601.194658	16.402842	-0.057000	3.690774
293.268757	4593.198902	16.407847	-0.056995	3.687722
293.211066	4585.224908	16.412851	-0.056979	3.684676
293.134926	4577.252233	16.417856	-0.056959	3.681626
293.240838	4569.234945	16.422861	-0.056973	3.678562
293.167202	4561.228114	16.427866	-0.056954	3.675495
293.060692	4553.212286	16.432871	-0.056929	3.672421
292.954664	4545.216211	16.437875	-0.056904	3.669351
292.743014	4537.202273	16.442880	-0.056859	3.666270
292.826602	4529.230506	16.447885	-0.056869	3.663210
292.860616	4521.245994	16.452890	-0.056870	3.660141
292.679849	4513.263273	16.457895	-0.056831	3.657064
292.883948	4505.232008	16.462899	-0.056864	3.653977
292.652943	4497.201500	16.467904	-0.056816	3.650875
292.674655	4489.258522	16.472909	-0.056814	3.647812
292.630048	4481.228962	16.477914	-0.056801	3.644710
292.616080	4473.292989	16.482919	-0.056793	3.641643
292.559299	4465.290819	16.487923	-0.056777	3.638547
292.449767	4457.285436	16.492928	-0.056751	3.635445
292.507210	4449.253610	16.497933	-0.056756	3.632335
292.390294	4441.254453	16.502938	-0.056729	3.629230
292.309648	4433.244392	16.507943	-0.056709	3.626119
292.481076	4425.266197	16.512947	-0.056735	3.623025
292.311348	4417.265694	16.517952	-0.056698	3.619910
292.196768	4409.325227	16.522957	-0.056672	3.616818
292.294519	4401.296498	16.527962	-0.056685	3.613694
292.269187	4393.268966	16.532967	-0.056675	3.610564
292.387339	4385.295035	16.537971	-0.056691	3.607457
292.166058	4377.285722	16.542976	-0.056645	3.604324
292.175754	4369.347669	16.547981	-0.056641	3.601222
292.278653	4361.360323	16.552986	-0.056655	3.598101
292.126123	4353.363898	16.557991	-0.056621	3.594966
292.047160	4345.359676	16.562995	-0.056601	3.591828
291.983570	4337.349446	16.568000	-0.056584	3.588685
292.050371	4329.353543	16.573005	-0.056591	3.585549
291.870463	4321.432536	16.578010	-0.056552	3.582432
291.759809	4313.388070	16.583015	-0.056526	3.579266
292.041136	4305.380907	16.588019	-0.056573	3.576123
291.911567	4297.381358	16.593024	-0.056544	3.572969
291.708420	4289.385619	16.598029	-0.056500	3.569811
291.810030	4281.407103	16.603034	-0.056514	3.566666
291.886149	4273.398741	16.608039	-0.056523	3.563505
291.921954	4265.426485	16.613043	-0.056524	3.560355
291.810611	4257.451655	16.618048	-0.056498	3.557197
291.628485	4249.430896	16.623053	-0.056459	3.554016
291.424077	4241.338752	16.628058	-0.056415	3.550803
291.292061	4233.372139	16.633063	-0.056385	3.547638
291.380394	4225.377359	16.638067	-0.056396	3.544467
291.418026	4217.421772	16.643072	-0.056398	3.541306
291.351150	4209.422288	16.648077	-0.056380	3.538123
291.170103	4201.422184	16.653082	-0.056341	3.534932
291.222835	4193.411728	16.658087	-0.056346	3.531742
291.534435	4185.392796	16.663091	-0.056398	3.528553
291.204094	4177.412527	16.668096	-0.056331	3.525357
291.412885	4169.470459	16.673101	-0.056365	3.522190
291.208828	4161.480341	16.678106	-0.056322	3.518989
291.174364	4153.501768	16.683111	-0.056310	3.515794
291.026039	4145.501816	16.688115	-0.056277	3.512584
290.953305	4137.469197	16.693120	-0.056258	3.509361
291.080854	4129.475202	16.698125	-0.056276	3.506156
290.974532	4121.510425	16.703130	-0.056251	3.502953
290.832890	4113.487433	16.708135	-0.056220	3.499722
290.771514	4105.578105	16.713139	-0.056203	3.496537
290.695066	4097.543961	16.718144	-0.056183	3.493298
290.944120	4089.498089	16.723149	-0.056224	3.490061
290.662321	4081.556011	16.728154	-0.056166	3.486847
290.608393	4073.554850	16.733159	-0.056151	3.483613
290.647863	4065.583130	16.738163	-0.056153	3.480390
290.620240	4057.596313	16.743168	-0.056142	3.477157
290.753735	4049.572628	16.748173	-0.056162	3.473911
290.685983	4041.553861	16.753178	-0.056144	3.470657
290.333949	4033.595983	16.758183	-0.056073	3.467416
290.507546	4025.566996	16.763187	-0.056100	3.464160
290.195923	4017.627949	16.768192	-0.056037	3.460921
290.249816	4009.637341	16.773197	-0.056041	3.457670
290.492237	4001.585492	16.778202	-0.056081	3.454398
290.446529	3993.601059	16.783207	-0.056067	3.451140
290.395257	3985.619288	16.788211	-0.056052	3.447881
290.083399	3977.650103	16.793216	-0.055989	3.444615
290.204047	3969.674211	16.798221	-0.056006	3.441357
290.283771	3961.661116	16.803226	-0.056015	3.438079
290.281996	3953.617326	16.808231	-0.056010	3.434783
289.950965	3945.684199	16.813235	-0.055943	3.431519
290.053305	3937.632141	16.818240	-0.055956	3.428217
290.007154	3929.639454	16.823245	-0.055943	3.424931
289.992977	3921.688254	16.828250	-0.055935	3.421660
290.067876	3913.661542	16.833255	-0.055943	3.418358
290.129761	3905.700421	16.838259	-0.055949	3.415079
289.797258	3897.709188	16.843264	-0.055882	3.411771
289.904559	3889.691672	16.848269	-0.055897	3.408464
289.821995	3881.742970	16.853274	-0.055876	3.405176
289.781058	3873.757790	16.858279	-0.055863	3.401871
289.865459	3865.778221	16.863283	-0.055873	3.398570
289.876471	3857.763579	16.868288	-0.055870	3.395248
289.718391	3849.706284	16.873293	-0.055835	3.391899
289.771873	3841.706109	16.878298	-0.055840	3.388578
289.727119	3833.725787	16.883303	-0.055826	3.385259
289.761200	3825.774405	16.888307	-0.055827	3.381951
289.395349	3817.797220	16.893312	-0.055754	3.378615
289.478239	3809.815468	16.898317	-0.055764	3.375290
289.436431	3801.809535	16.903322	-0.055751	3.371947
289.343745	3793.811421	16.908327	-0.055728	3.368602
289.480439	3785.831554	16.913331	-0.055748	3.365270
289.664408	3777.833122	16.918336	-0.055777	3.361928
289.489364	3769.862195	16.923341	-0.055739	3.358581
289.270873	3761.901547	16.928346	-0.055693	3.355234
289.404658	3753.832383	16.933351	-0.055712	3.351851
289.335247	3745.853449	16.938355	-0.055694	3.348495
289.280255	3737.856829	16.943360	-0.055679	3.345128
289.276351	3729.897199	16.948365	-0.055673	3.341776
289.371635	3721.914732	16.953370	-0.055685	3.338414
289.194920	3713.919605	16.958375	-0.055647	3.335034
288.919314	3705.959777	16.963379	-0.055590	3.331661
289.149026	3697.893808	16.968384	-0.055627	3.328259
288.997184	3689.925481	16.973389	-0.055594	3.324880
288.948103	3681.961451	16.978394	-0.055579	3.321504
289.038206	3673.955027	16.983399	-0.055591	3.318111
288.913162	3665.994861	16.988403	-0.055562	3.314726
288.743006	3657.952176	16.993408	-0.055525	3.311302
288.701531	3649.978356	16.998413	-0.055512	3.307907
288.701820	3641.958481	17.003418	-0.055507	3.304492
288.631497	3634.000765	17.008423	-0.055488	3.301096
288.681348	3626.034697	17.013427	-0.055492	3.297698
288.621121	3618.014363	17.018432	-0.055476	3.294269
288.445394	3610.028820	17.023437	-0.055437	3.290847
288.407448	3602.049495	17.028442	-0.055425	3.287429
288.510554	3594.033025	17.033447	-0.055439	3.283998
288.429936	3586.104747	17.038451	-0.055419	3.280593
288.332665	3578.114318	17.043456	-0.055395	3.277158
288.193479	3570.107811	17.048461	-0.055364	3.273710
288.321782	3562.085516	17.053466	-0.055382	3.270263
288.132119	3554.107082	17.058471	-0.055342	3.266818
288.248600	3546.116470	17.063475	-0.055358	3.263376
287.987488	3538.124663	17.068480	-0.055304	3.259915
288.068657	3530.170766	17.073485	-0.055314	3.256481
288.164998	3522.148107	17.078490	-0.055326	3.253013
288.279960	3514.097666	17.083495	-0.055342	3.249531
288.147971	3506.175719	17.088499	-0.055312	3.246091
287.912512	3498.197749	17.093504	-0.055263	3.242619
288.071760	3490.226379	17.098509	-0.055288	3.239161
287.948704	3482.252328	17.103514	-0.055259	3.235688
287.891919	3474.168959	17.108519	-0.055243	3.232166
287.920652	3466.188826	17.113523	-0.055243	3.228688
287.707910	3458.179757	17.118528	-0.055198	3.225184
287.856500	3450.207129	17.123533	-0.055221	3.221707
287.951900	3442.221627	17.128538	-0.055233	3.218219
287.798998	3434.226723	17.133543	-0.055199	3.214712
287.689355	3426.297776	17.138547	-0.055174	3.211232
287.533700	3418.288660	17.143552	-0.055139	3.207712
287.597554	3410.274067	17.148557	-0.055146	3.204194
287.654168	3402.337055	17.153562	-0.055151	3.200706
287.571810	3394.344596	17.158567	-0.055130	3.197184
287.392630	3386.365237	17.163571	-0.055091	3.193660
287.406066	3378.324093	17.168576	-0.055089	3.190113
287.455999	3370.342096	17.173581	-0.055093	3.186589
287.427505	3362.386993	17.178586	-0.055082	3.183070
287.078468	3354.411512	17.183591	-0.055012	3.179525
287.334289	3346.438411	17.188595	-0.055054	3.176002
287.191940	3338.407559	17.193600	-0.055022	3.172433
287.049528	3330.409709	17.198605	-0.054990	3.168875
287.158725	3322.426781	17.203610	-0.055005	3.165330
286.978410	3314.472362	17.208615	-0.054966	3.161781
287.103035	3306.482683	17.213619	-0.054984	3.158226
287.171386	3298.455660	17.218624	-0.054991	3.154647
287.169523	3290.436870	17.223629	-0.054986	3.151065
286.974304	3282.481655	17.228634	-0.054944	3.147499
286.748751	3274.487645	17.233639	-0.054897	3.143911
287.027922	3266.512603	17.238643	-0.054943	3.140348
287.032928	3258.529579	17.243648	-0.054939	3.136767
287.051986	3250.521647	17.248653	-0.054937	3.133170
286.907471	3242.563306	17.253658	-0.054905	3.129584
286.846998	3234.553196	17.258663	-0.054888	3.125975
286.801949	3226.612449	17.263667	-0.054874	3.122394
286.570618	3218.630167	17.268672	-0.054826	3.118781
286.605252	3210.648101	17.273677	-0.054827	3.115176
286.572926	3202.642607	17.278682	-0.054816	3.111553
286.493164	3194.619493	17.283687	-0.054795	3.107916
286.634624	3186.655282	17.288691	-0.054816	3.104311
286.509727	3178.668489	17.293696	-0.054788	3.100680
286.387660	3170.703879	17.298701	-0.054760	3.097055
286.504290	3162.700674	17.303706	-0.054776	3.093419
286.425844	3154.660708	17.308711	-0.054756	3.089752
286.432650	3146.740081	17.313715	-0.054752	3.086140
286.382347	3138.743617	17.318720	-0.054737	3.082487
286.496208	3130.768023	17.323725	-0.054753	3.078846
286.496266	3122.791538	17.328730	-0.054748	3.075195
286.030911	3114.710465	17.333735	-0.054656	3.071470
286.235219	3106.731733	17.338739	-0.054689	3.067819
286.087740	3098.752102	17.343744	-0.054656	3.064146
286.048858	3090.808327	17.348749	-0.054643	3.060491
285.965632	3082.846759	17.353754	-0.054622	3.056821
286.027777	3074.818969	17.358759	-0.054628	3.053123
286.071379	3066.834553	17.363763	-0.054631	3.049440
285.761782	3058.892765	17.368768	-0.054568	3.045755
285.686723	3050.925759	17.373773	-0.054549	3.042065
285.803759	3042.933784	17.378778	-0.054565	3.038368
285.616313	3034.950724	17.383783	-0.054525	3.034657
285.459853	3026.962222	17.388787	-0.054491	3.030939
285.522145	3018.952138	17.393792	-0.054497	3.027218
285.414074	3010.985702	17.398797	-0.054471	3.023504
285.442370	3002.995472	17.403802	-0.054471	3.019781
285.569693	2994.998714	17.408807	-0.054490	3.016055
285.646051	2987.004425	17.413811	-0.054499	3.012323
285.579172	2979.013026	17.418816	-0.054481	3.008581
285.350103	2971.050653	17.423821	-0.054433	3.004840
285.499530	2963.108351	17.428826	-0.054455	3.001122
285.431462	2955.112387	17.433831	-0.054437	2.997364
285.304415	2947.133387	17.438835	-0.054408	2.993606
285.349679	2939.093209	17.443840	-0.054411	2.989823
285.229987	2931.123707	17.448845	-0.054384	2.986061
285.165518	2923.162413	17.453850	-0.054366	2.982300
284.990207	2915.185364	17.458855	-0.054328	2.978521
285.013021	2907.204651	17.463859	-0.054327	2.974746
284.907820	2899.211519	17.468864	-0.054302	2.970954
284.759197	2891.229351	17.473869	-0.054269	2.967160
284.974886	2883.240080	17.478874	-0.054304	2.963376
284.797508	2875.262458	17.483879	-0.054266	2.959573
284.680255	2867.329334	17.488883	-0.054238	2.955789
284.815562	2859.289558	17.493888	-0.054258	2.951962
284.857173	2851.304892	17.498893	-0.054261	2.948152
284.737711	2843.329682	17.503898	-0.054233	2.944333
284.599361	2835.353896	17.508903	-0.054202	2.940508
284.715248	2827.390898	17.513907	-0.054218	2.936697
284.445235	2819.404745	17.518912	-0.054163	2.932850
284.451505	2811.412740	17.523917	-0.054158	2.929010
284.434427	2803.437005	17.528922	-0.054150	2.925171
284.330679	2795.463098	17.533927	-0.054125	2.921324
284.452906	2787.492456	17.538931	-0.054143	2.917485
284.286545	2779.480604	17.543936	-0.054106	2.913605
284.306276	2771.415197	17.548941	-0.054105	2.909705
284.410195	2763.450512	17.553946	-0.054119	2.905852
284.243215	2755.495992	17.558951	-0.054082	2.901985
284.305684	2747.540296	17.563955	-0.054088	2.898124
284.001821	2739.577349	17.568960	-0.054027	2.894235
283.883899	2731.588630	17.573965	-0.053999	2.890338
284.097995	2723.612888	17.578970	-0.054034	2.886460
284.013967	2715.625983	17.583975	-0.054013	2.882556
283.939359	2707.687179	17.588979	-0.053993	2.878670
283.850537	2699.677888	17.593984	-0.053972	2.874743
283.933408	2691.656564	17.598989	-0.053982	2.870815
284.014217	2683.678178	17.603994	-0.053991	2.866902
283.917926	2675.699428	17.608999	-0.053968	2.862974
284.061162	2667.729460	17.614003	-0.053989	2.859058
283.823549	2659.790453	17.619008	-0.053940	2.855131
283.549186	2651.812296	17.624013	-0.053883	2.851177
283.644435	2643.817463	17.629018	-0.053896	2.847230
283.551447	2635.837962	17.634023	-0.053873	2.843274
283.371962	2627.900823	17.639027	-0.053834	2.839329
283.471066	2619.912370	17.644032	-0.053847	2.835369
283.645314	2611.869364	17.649037	-0.053875	2.831380
283.320968	2603.935168	17.654042	-0.053809	2.827412
283.232558	2595.935284	17.659047	-0.053787	2.823418
283.332419	2587.955227	17.664051	-0.053800	2.819440
283.358364	2579.992976	17.669056	-0.053800	2.815461
283.078816	2572.029046	17.674061	-0.053742	2.811457
283.127754	2564.032006	17.679066	-0.053746	2.807451
283.032188	2556.040627	17.684071	-0.053723	2.803433
283.109094	2548.076849	17.689075	-0.053732	2.799433
283.069488	2540.108134	17.694080	-0.053719	2.795418
283.077847	2532.080377	17.699085	-0.053715	2.791370
283.181669	2524.113734	17.704090	-0.053729	2.787353
282.891384	2516.148761	17.709095	-0.053670	2.783308
283.059717	2508.186537	17.714099	-0.053696	2.779285
283.011116	2500.212428	17.719104	-0.053682	2.775238
282.863024	2492.243162	17.724109	-0.053649	2.771181
282.800265	2484.279966	17.729114	-0.053632	2.767126
282.872579	2476.266120	17.734119	-0.053640	2.763048
282.678716	2468.342364	17.739123	-0.053598	2.758994
282.719057	2460.354005	17.744128	-0.053600	2.754915
282.844768	2452.263767	17.749133	-0.053618	2.750782
282.615247	2444.348010	17.754138	-0.053570	2.746712
282.418247	2436.362472	17.759143	-0.053528	2.742602
282.680630	2428.400855	17.764147	-0.053572	2.738525
282.410936	2420.450930	17.769152	-0.053516	2.734416
282.309822	2412.458012	17.774157	-0.053492	2.730289
282.380792	2404.491227	17.779162	-0.053500	2.726180
282.357894	2396.524056	17.784167	-0.053490	2.722059
282.189880	2388.573008	17.789171	-0.053454	2.717931
282.265128	2380.566598	17.794176	-0.053462	2.713782
282.273208	2372.573812	17.799181	-0.053459	2.709631
282.433629	2364.596608	17.804186	-0.053483	2.705490
282.160551	2356.655391	17.809191	-0.053427	2.701335
282.292938	2348.686194	17.814195	-0.053446	2.697185
282.351118	2340.690967	17.819200	-0.053452	2.693009
282.194603	2332.702999	17.824205	-0.053417	2.688818
282.066930	2324.768120	17.829210	-0.053388	2.684649
282.156470	2316.780161	17.834215	-0.053399	2.680460
281.916534	2308.875979	17.839219	-0.053349	2.676287
281.848225	2300.844408	17.844224	-0.053331	2.672052
281.851685	2292.854135	17.849229	-0.053327	2.667836
281.790763	2284.897310	17.854234	-0.053310	2.663628
281.887265	2276.903846	17.859239	-0.053323	2.659403
281.650876	2268.981911	17.864243	-0.053273	2.655188
281.813109	2260.951093	17.869248	-0.053298	2.650934
281.600703	2253.010921	17.874253	-0.053253	2.646698
281.698854	2245.040217	17.879258	-0.053266	2.642458
281.599260	2237.077014	17.884263	-0.053242	2.638203
281.675502	2229.100990	17.889267	-0.053251	2.633945
281.625331	2221.104151	17.894272	-0.053236	2.629661
281.618114	2213.117975	17.899277	-0.053230	2.625379
281.598587	2205.175687	17.904282	-0.053221	2.621113
281.429506	2197.222813	17.909287	-0.053184	2.616823
281.330459	2189.252966	17.914291	-0.053160	2.612523
281.323545	2181.262600	17.919296	-0.053154	2.608210
281.067211	2173.320520	17.924301	-0.053100	2.603899
280.988201	2165.382030	17.929306	-0.053080	2.599596
281.033511	2157.396068	17.934311	-0.053084	2.595267
281.015086	2149.251362	17.939315	-0.053075	2.590841
280.799417	2141.292867	17.944320	-0.053029	2.586495
280.847209	2133.338875	17.949325	-0.053033	2.582162
280.994423	2125.392287	17.954330	-0.053055	2.577833
280.767705	2117.461782	17.959335	-0.053007	2.573480
280.757501	2109.498200	17.964339	-0.053000	2.569116
280.635013	2101.534180	17.969344	-0.052972	2.564737
280.628955	2093.591252	17.974349	-0.052965	2.560369
280.623375	2085.646238	17.979354	-0.052959	2.555994
280.569016	2077.648350	17.984359	-0.052944	2.551578
280.719777	2069.661728	17.989363	-0.052966	2.547175
280.656527	2061.696582	17.994368	-0.052949	2.542761
280.562772	2053.756775	17.999373	-0.052926	2.538352
280.530317	2045.803068	18.004378	-0.052915	2.533931
280.340824	2037.821085	18.009383	-0.052874	2.529476
280.341954	2029.867790	18.014387	-0.052869	2.525042
280.346915	2021.905344	18.019392	-0.052865	2.520596
280.399413	2013.938855	18.024397	-0.052869	2.516143
280.422506	2005.938166	18.029402	-0.052868	2.511661
280.058662	1997.986515	18.034407	-0.052795	2.507170
280.094763	1990.026918	18.039411	-0.052796	2.502696
280.205649	1982.047795	18.044416	-0.052812	2.498209
280.120122	1974.092567	18.049421	-0.052791	2.493712
279.989521	1966.141019	18.054426	-0.052761	2.489206
279.942710	1958.157296	18.059431	-0.052747	2.484680
279.952030	1950.236917	18.064435	-0.052743	2.480185
279.924345	1942.267667	18.069440	-0.052733	2.475652
279.728120	1934.292801	18.074445	-0.052691	2.471095
279.626744	1926.352097	18.079450	-0.052667	2.466556
279.624827	1918.371346	18.084455	-0.052661	2.461993
279.855310	1910.399501	18.089459	-0.052699	2.457444
279.629132	1902.441733	18.094464	-0.052651	2.452860
279.466171	1894.476579	18.099469	-0.052615	2.448269
279.642860	1886.514887	18.104474	-0.052643	2.443696
279.574562	1878.554800	18.109479	-0.052625	2.439097
279.579582	1870.605499	18.114483	-0.052621	2.434501
279.371196	1862.572009	18.119488	-0.052576	2.429832
279.343944	1854.613992	18.124493	-0.052566	2.425211
279.232174	1846.693866	18.129498	-0.052540	2.420597
279.148240	1838.739980	18.134503	-0.052519	2.415956
279.448973	1830.734619	18.139507	-0.052569	2.411306
279.198863	1822.795829	18.144512	-0.052518	2.406644
279.134733	1814.857409	18.149517	-0.052500	2.401987
279.171410	1806.927889	18.154522	-0.052502	2.397334
279.001230	1798.944579	18.159527	-0.052465	2.392624
279.072013	1790.978751	18.164531	-0.052473	2.387934
279.054088	1782.997878	18.169536	-0.052464	2.383219
278.704521	1775.098862	18.174541	-0.052394	2.378517
278.973460	1767.120306	18.179546	-0.052438	2.373808
278.793144	1759.151117	18.184551	-0.052399	2.369058
278.795039	1751.203875	18.189555	-0.052394	2.364327
278.770852	1743.253303	18.194560	-0.052385	2.359583
278.605836	1735.336174	18.199565	-0.052349	2.354837
278.685488	1727.314023	18.204570	-0.052358	2.350039
278.581793	1719.354842	18.209575	-0.052333	2.345253
278.461090	1711.419715	18.214579	-0.052306	2.340472
278.541598	1703.459843	18.219584	-0.052315	2.335681
278.450735	1695.502092	18.224589	-0.052293	2.330868
278.349094	1687.562294	18.229594	-0.052269	2.326056
278.247951	1679.622459	18.234599	-0.052245	2.321233
278.550657	1671.644815	18.239603	-0.052296	2.316410
278.456429	1663.675353	18.244608	-0.052273	2.311550
278.151674	1655.742841	18.249613	-0.052211	2.306684
278.125721	1647.810201	18.254618	-0.052200	2.301831
278.138348	1639.835559	18.259623	-0.052197	2.296945
278.095237	1631.894922	18.264627	-0.052184	2.292066
278.032281	1623.943286	18.269632	-0.052167	2.287167
277.970465	1616.002491	18.274637	-0.052150	2.282264
278.056209	1608.058415	18.279642	-0.052161	2.277362
277.884884	1600.057908	18.284647	-0.052124	2.272392
277.876420	1592.083608	18.289651	-0.052117	2.267441
277.746284	1584.148851	18.294656	-0.052087	2.262494
277.575868	1576.217862	18.299661	-0.052050	2.257534
277.776992	1568.258489	18.304666	-0.052082	2.252578
277.519995	1560.311288	18.309671	-0.052029	2.247579
277.525792	1552.371879	18.314675	-0.052025	2.242597
277.648751	1544.431510	18.319680	-0.052042	2.237613
277.495973	1536.476293	18.324685	-0.052009	2.232584
277.635482	1528.508293	18.329690	-0.052029	2.227562
277.456835	1520.570988	18.334695	-0.051991	2.222520
277.492652	1512.647497	18.339699	-0.051992	2.217494
277.354228	1504.700489	18.344704	-0.051961	2.212426
277.110826	1496.761362	18.349709	-0.051910	2.207342
277.258708	1488.826276	18.354714	-0.051932	2.202284
277.151321	1480.888857	18.359719	-0.051907	2.197190
277.026861	1472.941722	18.364723	-0.051879	2.192076
276.964924	1464.975768	18.369728	-0.051862	2.186944
276.953301	1457.020928	18.374733	-0.051854	2.181811
277.033440	1449.084075	18.379738	-0.051864	2.176687
276.851615	1441.149178	18.384743	-0.051825	2.171527
277.259289	1433.151532	18.389747	-0.051895	2.166369
277.133137	1425.246292	18.394752	-0.051866	2.161209
276.752038	1417.358881	18.399757	-0.051790	2.156025
276.994290	1409.370429	18.404762	-0.051830	2.150820
276.917222	1401.423508	18.409767	-0.051810	2.145600
276.732785	1393.523913	18.414771	-0.051771	2.140388
276.561360	1385.604200	18.419776	-0.051733	2.135152
276.727089	1377.614777	18.424781	-0.051759	2.129888
276.560850	1369.725425	18.429786	-0.051723	2.124647
276.217911	1361.819114	18.434791	-0.051653	2.119363
276.313414	1353.856408	18.439795	-0.051666	2.114072
276.297854	1345.836146	18.444800	-0.051658	2.108717
276.150785	1337.918873	18.449805	-0.051625	2.103406
275.990859	1330.029825	18.454810	-0.051590	2.098098
276.037483	1322.065286	18.459815	-0.051593	2.092747
276.018470	1314.133368	18.464819	-0.051584	2.087397
275.774079	1306.237241	18.469824	-0.051534	2.082036
275.848021	1298.296879	18.474829	-0.051542	2.076662
275.810489	1290.349186	18.479834	-0.051530	2.071258
275.726017	1282.391790	18.484839	-0.051509	2.065829
275.820174	1274.469424	18.489843	-0.051521	2.060427
275.956892	1266.528048	18.494848	-0.051541	2.055002
275.762937	1258.600566	18.499853	-0.051500	2.049539
275.645870	1250.704351	18.504858	-0.051472	2.044091
275.385397	1242.807189	18.509863	-0.051419	2.038613
275.490625	1234.865480	18.514867	-0.051433	2.033126
275.216137	1226.937914	18.519872	-0.051376	2.027596
275.268010	1218.977989	18.524877	-0.051381	2.022062
275.567265	1211.035877	18.529882	-0.051431	2.016550
275.389823	1203.106173	18.534887	-0.051393	2.010982
275.168495	1195.222592	18.539891	-0.051346	2.005427
275.251398	1187.282012	18.544896	-0.051356	1.999848
275.112333	1179.383412	18.549901	-0.051325	1.994260
275.318027	1171.412841	18.554906	-0.051358	1.988641
275.166818	1163.503219	18.559911	-0.051325	1.983012
275.071344	1155.613103	18.564915	-0.051302	1.977387
275.096211	1147.666815	18.569920	-0.051301	1.971718
274.849644	1139.771249	18.574925	-0.051250	1.966041
274.833577	1131.865922	18.579930	-0.051241	1.960364
274.607134	1123.969083	18.584935	-0.051194	1.954655
274.663384	1115.978818	18.589939	-0.051199	1.948892
274.566950	1108.063450	18.594944	-0.051176	1.943149
274.460199	1100.161493	18.599949	-0.051151	1.937398
274.482691	1092.227655	18.604954	-0.051150	1.931621
274.478001	1084.297922	18.609959	-0.051143	1.925826
274.681605	1076.371014	18.614963	-0.051176	1.920039
274.649398	1068.481172	18.619968	-0.051165	1.914236
274.365408	1060.573864	18.624973	-0.051106	1.908374
274.460623	1052.648575	18.629978	-0.051119	1.902523
274.330526	1044.762611	18.634983	-0.051089	1.896658
274.238022	1036.861898	18.639987	-0.051067	1.890768
274.064037	1028.970054	18.644992	-0.051029	1.884856
274.110076	1021.060425	18.649997	-0.051032	1.878938
274.249468	1013.133194	18.655002	-0.051053	1.872999
273.933622	1005.233021	18.660007	-0.050989	1.867009
273.995729	997.313458	18.665011	-0.050995	1.861028
273.919877	989.430715	18.670016	-0.050976	1.855041
273.996554	981.487413	18.675021	-0.050985	1.849005
274.114474	973.579742	18.680026	-0.051001	1.842982
274.053296	965.696192	18.685031	-0.050985	1.836936
273.920211	957.803025	18.690035	-0.050955	1.830855
273.969136	949.884693	18.695040	-0.050958	1.824755
273.875991	942.010022	18.700045	-0.050936	1.818652
273.628131	934.162020	18.705050	-0.050884	1.812530
273.486902	926.245402	18.710055	-0.050853	1.806347
273.638134	918.341028	18.715059	-0.050876	1.800188
273.500943	910.468471	18.720064	-0.050845	1.793997
273.253068	902.534797	18.725069	-0.050793	1.787723
273.384732	894.629800	18.730074	-0.050813	1.781496
273.553219	886.713515	18.735079	-0.050839	1.775244
273.373262	878.843705	18.740083	-0.050800	1.768962
273.137233	870.998605	18.745088	-0.050751	1.762672
273.088221	863.119620	18.750093	-0.050736	1.756354
273.077286	855.215348	18.755098	-0.050729	1.749999
273.169057	847.300894	18.760103	-0.050741	1.743625
273.155781	839.436509	18.765107	-0.050733	1.737255
273.043834	831.559662	18.770112	-0.050707	1.730838
272.831458	823.700729	18.775117	-0.050662	1.724400
272.959129	815.828875	18.780122	-0.050681	1.717970
272.683727	807.960477	18.785127	-0.050624	1.711467
272.608065	800.075802	18.790131	-0.050605	1.704952
272.636987	792.206101	18.795136	-0.050605	1.698438
272.635792	784.303432	18.800141	-0.050599	1.691867
272.482727	776.452628	18.805146	-0.050565	1.685294
272.262364	768.622567	18.810151	-0.050519	1.678704
272.295808	760.740768	18.815155	-0.050520	1.672077
272.448603	752.816758	18.820160	-0.050543	1.665405
272.325267	744.975153	18.825165	-0.050515	1.658739
272.354974	737.113338	18.830170	-0.050515	1.652049
272.060777	729.262895	18.835175	-0.050455	1.645298
272.065265	721.428126	18.840179	-0.050451	1.638573
271.923277	713.541128	18.845184	-0.050419	1.631755
272.101268	705.611361	18.850189	-0.050447	1.624916
271.888640	697.809508	18.855194	-0.050402	1.618105
271.742072	689.951199	18.860199	-0.050369	1.611225
271.860992	682.087142	18.865203	-0.050386	1.604348
271.728803	674.274830	18.870208	-0.050356	1.597451
271.621477	666.409888	18.875213	-0.050331	1.590481
271.536802	658.578098	18.880218	-0.050310	1.583513
271.470677	650.738171	18.885223	-0.050293	1.576510
271.436670	642.883742	18.890227	-0.050281	1.569467
271.515163	635.035450	18.895232	-0.050290	1.562414
271.405677	627.218734	18.900237	-0.050265	1.555330
271.309854	619.375787	18.905242	-0.050242	1.548192
271.101354	611.554539	18.910247	-0.050198	1.541024
271.186745	603.711759	18.915251	-0.050208	1.533847
271.107372	595.891708	18.920256	-0.050188	1.526632
270.829418	588.101400	18.925261	-0.050131	1.519380
271.044714	580.231821	18.930266	-0.050166	1.512095
270.899326	572.410660	18.935271	-0.050134	1.504764
270.885649	564.601040	18.940275	-0.050126	1.497429
270.759424	556.791407	18.945280	-0.050097	1.490040
270.728370	548.976419	18.950285	-0.050086	1.482624
270.725722	541.181930	18.955290	-0.050080	1.475195
270.505667	533.331428	18.960295	-0.050034	1.467640
270.505337	525.525691	18.965299	-0.050029	1.460124
270.634096	517.702461	18.970304	-0.050048	1.452573
270.344770	509.927500	18.975309	-0.049989	1.444962
270.152820	502.183276	18.980314	-0.049948	1.437356
270.120447	494.363435	18.985319	-0.049936	1.429662
270.245491	486.545918	18.990323	-0.049954	1.421954
270.183228	478.777996	18.995328	-0.049938	1.414222
270.219959	470.960118	19.000333	-0.049939	1.406415
270.290571	463.192725	19.005338	-0.049947	1.398620
270.108213	455.425066	19.010343	-0.049908	1.390739
270.035217	447.654748	19.015347	-0.049889	1.382829
269.983980	439.887634	19.020352	-0.049874	1.374880
269.877901	432.115469	19.025357	-0.049849	1.366870
269.796559	424.379330	19.030362	-0.049829	1.358854
269.738973	416.607210	19.035367	-0.049813	1.350758
269.510944	408.886606	19.040371	-0.049766	1.342637
269.570795	401.117451	19.045376	-0.049771	1.334466
269.490185	393.359096	19.050381	-0.049751	1.326231
269.500045	385.636207	19.055386	-0.049748	1.317999
269.244610	377.819190	19.060391	-0.049695	1.309565
269.248712	370.042273	19.065395	-0.049691	1.301168
269.302398	362.320222	19.070400	-0.049695	1.292785
269.006178	354.628629	19.075405	-0.049635	1.284316
269.015021	346.926941	19.080410	-0.049632	1.275837
269.094603	339.179076	19.085415	-0.049641	1.267262
268.970401	331.495122	19.090419	-0.049613	1.258662
268.739723	323.827779	19.095424	-0.049565	1.250002
268.753938	316.110699	19.100429	-0.049562	1.241271
268.770255	308.429257	19.105434	-0.049560	1.232520
268.515731	300.755952	19.110439	-0.049508	1.223663
268.369526	293.093372	19.115443	-0.049475	1.214774
268.417948	285.393450	19.120448	-0.049479	1.205816
268.129459	277.775932	19.125453	-0.049420	1.196819
268.186964	270.085761	19.130458	-0.049426	1.187738
268.079888	262.441303	19.135463	-0.049401	1.178609
267.822256	254.825208	19.140467	-0.049348	1.169411
267.769759	247.186050	19.145472	-0.049333	1.160154
267.681314	239.540385	19.150477	-0.049311	1.150808
267.670482	231.883648	19.155482	-0.049304	1.141388
267.407215	224.290743	19.160487	-0.049250	1.131915
267.354653	216.677449	19.165491	-0.049235	1.122382
267.357326	209.069377	19.170496	-0.049230	1.112785
267.150527	201.488414	19.175501	-0.049187	1.103094
267.211643	193.889087	19.180506	-0.049193	1.093353
267.091975	186.317025	19.185511	-0.049166	1.083518
267.055007	178.761953	19.190515	-0.049154	1.073635
266.959808	171.197387	19.195520	-0.049131	1.063634
266.663207	163.689363	19.200525	-0.049071	1.053567
266.654337	156.138180	19.205530	-0.049064	1.043412
266.402980	148.653003	19.210535	-0.049012	1.033190
266.449511	141.111581	19.215539	-0.049016	1.022859
266.323674	133.625182	19.220544	-0.048987	1.012458
266.369068	126.116682	19.225549	-0.048991	1.001959
266.117707	118.670064	19.230554	-0.048939	0.991364
265.985093	111.188879	19.235559	-0.048909	0.980634
265.904318	103.739726	19.240563	-0.048889	0.969845
265.713950	96.329450	19.245568	-0.048849	0.958964
265.633601	88.900714	19.250573	-0.048829	0.947959
265.550303	81.506155	19.255578	-0.048808	0.936875
265.484958	74.109735	19.260583	-0.048791	0.925660
265.224783	66.778551	19.265587	-0.048738	0.914356
265.253475	59.625814	19.270592	-0.048738	0.903268