Fri Mar 12 11:40:20 2021


Number of Points = 3626

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
-0.247271	0.147060	0.000000	0.000107	0.719844
0.060485	0.123379	0.005005	0.000049	0.719906
0.044593	0.126841	0.010010	0.000053	0.719907
-0.066015	0.144279	0.015014	0.000073	0.719902
0.094345	0.120986	0.020019	0.000043	0.719912
-0.022423	0.070889	0.025024	0.000065	0.719772
0.071260	-0.028631	0.030029	0.000048	0.719609
0.072073	-0.028936	0.035034	0.000048	0.719609
-0.128421	0.005343	0.040038	0.000085	0.719606
0.195988	-0.049663	0.045043	0.000025	0.719611
0.063396	-0.031119	0.050048	0.000050	0.719601
0.120292	-0.038602	0.055053	0.000039	0.719606
0.081844	-0.031440	0.060058	0.000046	0.719606
0.013638	-0.021512	0.065062	0.000059	0.719602
0.225749	-0.054222	0.070067	0.000020	0.719612
0.202322	-0.053695	0.075072	0.000024	0.719604
0.124250	-0.038367	0.080077	0.000039	0.719607
0.260799	-0.069260	0.085082	0.000014	0.719594
-0.057709	-0.174583	0.090086	0.000073	0.719274
-0.006411	-0.178695	0.095091	0.000064	0.719284
0.010303	-0.188164	0.100096	0.000061	0.719271
-0.083295	-0.167263	0.105101	0.000078	0.719279
-0.012688	-0.182728	0.110106	0.000065	0.719273
-0.139086	-0.161960	0.115110	0.000089	0.719270
-0.096245	-0.215335	0.120115	0.000081	0.719179
-0.111103	-0.322987	0.125120	0.000084	0.718962
-0.019907	-0.336897	0.130125	0.000067	0.718966
-0.048668	-0.331777	0.135130	0.000072	0.718966
-0.208325	-0.306390	0.140134	0.000102	0.718960
-0.058981	-0.354072	0.145139	0.000074	0.718918
-0.254783	-0.457372	0.150144	0.000111	0.718645
-0.016430	-0.496940	0.155149	0.000067	0.718651
-0.015065	-0.498687	0.160154	0.000066	0.718647
0.059137	-0.512142	0.165158	0.000053	0.718647
0.085963	-0.648678	0.170163	0.000048	0.718387
-0.039613	-0.642874	0.175168	0.000071	0.718354
0.016888	-0.650647	0.180173	0.000061	0.718358
0.056349	-0.697355	0.185178	0.000054	0.718280
-0.123589	-0.797036	0.190182	0.000087	0.718019
-0.079684	-0.800908	0.195187	0.000079	0.718027
-0.096582	-0.801850	0.200192	0.000082	0.718019
-0.229815	-0.909998	0.205197	0.000107	0.717758
-0.230015	-0.934328	0.210202	0.000108	0.717710
-0.005869	-0.977295	0.215206	0.000066	0.717704
-0.194534	-1.050840	0.220211	0.000101	0.717492
-0.265783	-1.094200	0.225216	0.000115	0.717381
-0.079541	-1.122679	0.230221	0.000080	0.717390
-0.043268	-1.243819	0.235226	0.000073	0.717163
-0.221507	-1.249870	0.240230	0.000107	0.717088
-0.345702	-1.225027	0.245235	0.000130	0.717093
-0.551509	-1.355173	0.250240	0.000168	0.716763
-0.471716	-1.370019	0.255245	0.000154	0.716761
-0.343681	-1.433915	0.260250	0.000130	0.716680
-0.355753	-1.549601	0.265254	0.000132	0.716447
-0.464898	-1.526219	0.270259	0.000153	0.716454
-0.439990	-1.646209	0.275264	0.000148	0.716225
-0.334764	-1.709873	0.280269	0.000129	0.716136
-0.369642	-1.740420	0.285274	0.000135	0.716063
-0.540493	-1.801529	0.290278	0.000167	0.715882
-0.404753	-1.820395	0.295283	0.000142	0.715892
-0.547924	-1.963463	0.300288	0.000169	0.715558
-0.836681	-1.913284	0.305293	0.000223	0.715555
-0.801478	-2.024218	0.310298	0.000216	0.715347
-1.056654	-2.036137	0.315302	0.000264	0.715233
-1.704912	-1.965075	0.320307	0.000385	0.715145
-2.308151	-1.977508	0.325312	0.000497	0.714907
-2.029896	-2.024013	0.330317	0.000445	0.714913
-2.391949	-2.054445	0.335322	0.000513	0.714724
-3.374829	-1.937255	0.340326	0.000696	0.714609
-2.986337	-2.001987	0.345331	0.000624	0.714618
-3.425275	-2.050473	0.350336	0.000705	0.714366
-4.357146	-1.926933	0.355341	0.000879	0.714282
-3.889918	-2.010293	0.360346	0.000792	0.714281
-4.202098	-2.030781	0.365350	0.000850	0.714130
-5.187937	-1.930170	0.370355	0.001034	0.713981
-4.766019	-2.010840	0.375360	0.000956	0.713970
-4.999356	-1.964439	0.380365	0.000999	0.713979
-5.491557	-2.013284	0.385370	0.001091	0.713708
-5.746227	-1.994608	0.390374	0.001138	0.713654
-5.793995	-1.982919	0.395379	0.001147	0.713661
-6.065725	-1.939650	0.400384	0.001198	0.713650
-6.095082	-2.048759	0.405389	0.001203	0.713423
-6.432841	-2.016915	0.410394	0.001266	0.713366
-6.848607	-1.944370	0.415398	0.001344	0.713363
-6.700965	-1.967027	0.420403	0.001316	0.713370
-6.760474	-2.033723	0.425408	0.001328	0.713216
-7.537933	-1.988797	0.430413	0.001473	0.713030
-7.695893	-1.960654	0.435418	0.001502	0.713030
-8.049425	-1.900215	0.440422	0.001568	0.713024
-7.479589	-1.996530	0.445427	0.001462	0.713035
-7.703023	-2.042802	0.450432	0.001504	0.712863
-9.171970	-1.855565	0.455437	0.001777	0.712715
-8.386930	-1.994189	0.460442	0.001631	0.712717
-8.498460	-1.978434	0.465446	0.001652	0.712709
-8.758835	-1.926044	0.470451	0.001700	0.712720
-8.425569	-1.993581	0.475456	0.001639	0.712704
-9.021358	-2.043299	0.480461	0.001750	0.712393
-9.528942	-1.951408	0.485466	0.001844	0.712396
-9.811574	-1.905124	0.490470	0.001897	0.712388
-9.174580	-2.014042	0.495475	0.001778	0.712397
-9.882049	-1.893510	0.500480	0.001910	0.712386
-9.931594	-1.881117	0.505485	0.001919	0.712393
-9.909548	-2.029020	0.510490	0.001915	0.712106
-10.396618	-1.949479	0.515494	0.002006	0.712091
-10.971632	-1.842046	0.520499	0.002113	0.712101
-10.613479	-1.908920	0.525504	0.002047	0.712095
-10.341373	-1.956781	0.530509	0.001996	0.712096
-10.336599	-1.954969	0.535514	0.001995	0.712101
-10.910908	-1.956219	0.540518	0.002102	0.711894
-11.511511	-1.910237	0.545523	0.002214	0.711772
-11.238766	-1.962989	0.550528	0.002164	0.711764
-11.370536	-1.937200	0.555533	0.002188	0.711768
-11.409844	-1.929414	0.560538	0.002196	0.711770
-11.120743	-1.985354	0.565542	0.002142	0.711761
-11.126315	-2.000766	0.570547	0.002143	0.711728
-12.099055	-1.964613	0.575552	0.002324	0.711454
-11.921895	-1.993913	0.580557	0.002291	0.711459
-12.363215	-1.914609	0.585562	0.002373	0.711460
-12.585354	-1.876943	0.590566	0.002415	0.711456
-11.731093	-2.025530	0.595571	0.002256	0.711463
-12.220234	-1.942634	0.600576	0.002347	0.711454
-12.648578	-1.957508	0.605581	0.002427	0.711272
-13.070784	-1.947049	0.610586	0.002506	0.711143
-12.809609	-1.997737	0.615590	0.002457	0.711134
-12.902833	-1.973343	0.620595	0.002475	0.711150
-13.561789	-1.861434	0.625600	0.002597	0.711139
-12.962616	-1.965469	0.630605	0.002486	0.711144
-12.696791	-2.012292	0.635610	0.002436	0.711145
-13.748439	-1.951162	0.640614	0.002632	0.710893
-13.659559	-1.973297	0.645619	0.002616	0.710880
-13.827849	-1.945693	0.650624	0.002647	0.710875
-13.715248	-1.964783	0.655629	0.002626	0.710877
-13.705479	-1.965743	0.660634	0.002625	0.710878
-13.902067	-1.933409	0.665638	0.002661	0.710873
-13.734920	-2.038528	0.670643	0.002630	0.710722
-15.116154	-1.887437	0.675648	0.002887	0.710532
-14.573112	-1.979874	0.680653	0.002786	0.710541
-14.595488	-1.975340	0.685658	0.002791	0.710542
-15.054734	-1.898151	0.690662	0.002876	0.710532
-14.491036	-1.993136	0.695667	0.002771	0.710543
-14.507412	-1.993462	0.700672	0.002775	0.710536
-15.174492	-1.991134	0.705677	0.002899	0.710303
-15.808519	-1.917051	0.710682	0.003017	0.710225
-15.599751	-1.958280	0.715686	0.002978	0.710217
-15.355741	-1.997196	0.720691	0.002933	0.710226
-15.969972	-1.890938	0.725696	0.003047	0.710220
-15.420798	-1.987870	0.730701	0.002945	0.710221
-15.165774	-2.031639	0.735706	0.002898	0.710225
-16.326356	-1.979609	0.740710	0.003114	0.709915
-16.785991	-1.903358	0.745715	0.003200	0.709904
-16.619036	-1.937056	0.750720	0.003169	0.709895
-16.462918	-1.964684	0.755725	0.003140	0.709896
-16.409523	-1.973186	0.760730	0.003130	0.709898
-16.707681	-1.922277	0.765734	0.003185	0.709893
-16.206007	-2.005983	0.770739	0.003092	0.709904
-16.948920	-1.998456	0.775744	0.003230	0.709654
-17.520378	-1.924556	0.780749	0.003337	0.709598
-17.236491	-1.972731	0.785754	0.003284	0.709603
-17.495957	-1.930354	0.790758	0.003332	0.709595
-17.415290	-1.939736	0.795763	0.003318	0.709605
-17.117124	-1.996583	0.800768	0.003262	0.709597
-17.245769	-1.974633	0.805773	0.003286	0.709595
-17.779466	-2.038932	0.810778	0.003386	0.709276
-18.214924	-1.966395	0.815782	0.003467	0.709266
-18.087215	-1.985607	0.820787	0.003443	0.709273
-18.352182	-1.941623	0.825792	0.003492	0.709266
-18.622257	-1.892165	0.830797	0.003543	0.709269
-18.191335	-1.967483	0.835802	0.003463	0.709272
-18.362816	-1.940472	0.840806	0.003495	0.709264
-18.825358	-1.997293	0.845811	0.003581	0.708985
-19.257997	-1.935665	0.850816	0.003662	0.708954
-19.015834	-1.974849	0.855821	0.003617	0.708962
-19.170461	-1.947174	0.860826	0.003645	0.708962
-19.313029	-1.925821	0.865830	0.003672	0.708954
-18.891846	-1.995741	0.870835	0.003594	0.708964
-19.080267	-1.966098	0.875840	0.003629	0.708956
-19.708156	-2.005388	0.880845	0.003746	0.708653
-19.704668	-2.011037	0.885850	0.003745	0.708643
-20.427268	-1.885328	0.890854	0.003880	0.708637
-19.970499	-1.961556	0.895859	0.003795	0.708647
-19.874258	-1.980736	0.900864	0.003777	0.708643
-20.032065	-1.951403	0.905869	0.003807	0.708645
-19.979889	-1.963314	0.910874	0.003797	0.708639
-20.691576	-1.981207	0.915878	0.003930	0.708349
-20.474879	-2.014182	0.920883	0.003889	0.708360
-21.238165	-1.882971	0.925888	0.004031	0.708351
-21.245721	-1.878898	0.930893	0.004033	0.708356
-20.831334	-1.949640	0.935898	0.003956	0.708362
-21.211909	-1.886406	0.940902	0.004027	0.708353
-21.074508	-1.906300	0.945907	0.004001	0.708362
-21.179396	-2.000900	0.950912	0.004021	0.708135
-22.033599	-1.907444	0.955917	0.004180	0.708016
-21.793152	-1.947186	0.960922	0.004135	0.708023
-22.078842	-1.902340	0.965926	0.004189	0.708010
-21.806897	-1.945400	0.970931	0.004138	0.708021
-21.846791	-1.941561	0.975936	0.004146	0.708014
-22.026810	-1.908658	0.980941	0.004179	0.708016
-21.706672	-2.035285	0.985946	0.004120	0.707876
-22.903029	-1.912495	0.990950	0.004342	0.707695
-22.837696	-1.916592	0.995955	0.004330	0.707710
-22.788344	-1.927179	1.000960	0.004321	0.707706
-22.770846	-1.930260	1.005965	0.004318	0.707706
-22.582126	-1.962964	1.010970	0.004283	0.707707
-22.721236	-1.943501	1.015974	0.004309	0.707697
-22.563336	-2.036004	1.020979	0.004280	0.707567
-23.732115	-1.922946	1.025984	0.004497	0.707376
-23.638960	-1.938812	1.030989	0.004480	0.707377
-23.380635	-1.981980	1.035994	0.004432	0.707383
-23.713595	-1.927883	1.040998	0.004494	0.707372
-23.676977	-1.929627	1.046003	0.004487	0.707382
-23.797367	-1.910541	1.051008	0.004510	0.707377
-23.771704	-1.963460	1.056013	0.004505	0.707280
-24.628010	-1.907143	1.061018	0.004665	0.707086
-24.672583	-1.902503	1.066022	0.004673	0.707079
-24.383547	-1.949320	1.071027	0.004619	0.707089
-24.350338	-1.958506	1.076032	0.004613	0.707082
-24.461201	-1.939212	1.081037	0.004634	0.707081
-24.284042	-1.968069	1.086042	0.004601	0.707086
-24.413764	-2.005204	1.091046	0.004625	0.706965
-25.443155	-1.923077	1.096051	0.004817	0.706761
-25.242694	-1.962852	1.101056	0.004780	0.706753
-25.289325	-1.954152	1.106061	0.004789	0.706754
-25.309341	-1.948370	1.111066	0.004792	0.706758
-25.671411	-1.887833	1.116070	0.004860	0.706750
-25.347194	-1.939992	1.121075	0.004800	0.706761
-25.390391	-1.975968	1.126080	0.004808	0.706673
-26.610915	-1.871181	1.131085	0.005035	0.706446
-26.122158	-1.955742	1.136090	0.004944	0.706451
-26.281538	-1.931644	1.141094	0.004974	0.706442
-26.127602	-1.954657	1.146099	0.004945	0.706451
-26.181970	-1.947995	1.151104	0.004956	0.706445
-26.141800	-1.955157	1.156109	0.004948	0.706445
-26.037022	-2.022811	1.161114	0.004929	0.706346
-27.513210	-1.869206	1.166118	0.005204	0.706126
-26.808187	-1.988945	1.171123	0.005073	0.706138
-27.005213	-1.957589	1.176128	0.005109	0.706130
-27.311058	-1.902837	1.181133	0.005166	0.706130
-26.963821	-1.962950	1.186138	0.005102	0.706134
-27.255692	-1.912785	1.191142	0.005156	0.706130
-27.366461	-1.916683	1.196147	0.005177	0.706082
-27.916156	-1.926598	1.201152	0.005279	0.705865
-27.685519	-1.966937	1.206157	0.005236	0.705866
-27.715335	-1.959759	1.211162	0.005242	0.705870
-28.138242	-1.888446	1.216166	0.005321	0.705862
-27.819576	-1.939820	1.221171	0.005262	0.705872
-27.762928	-1.951355	1.226176	0.005251	0.705869
-28.058746	-1.988064	1.231181	0.005306	0.705689
-28.753464	-1.940294	1.236186	0.005436	0.705536
-28.599053	-1.973290	1.241190	0.005407	0.705525
-28.858006	-1.922202	1.246195	0.005455	0.705535
-28.921832	-1.914548	1.251200	0.005467	0.705527
-28.613173	-1.969844	1.256205	0.005410	0.705526
-28.452413	-1.997300	1.261210	0.005380	0.705529
-29.513199	-1.944085	1.266214	0.005578	0.705255
-29.635645	-1.942767	1.271219	0.005601	0.705213
-29.569141	-1.955864	1.276224	0.005588	0.705211
-29.688153	-1.934493	1.281229	0.005611	0.705211
-29.672201	-1.935554	1.286234	0.005608	0.705214
-29.894038	-1.900078	1.291238	0.005649	0.705206
-29.592620	-1.948656	1.296243	0.005593	0.705216
-30.003171	-1.999318	1.301248	0.005670	0.704967
-30.750240	-1.905508	1.306253	0.005809	0.704887
-30.509642	-1.943752	1.311258	0.005764	0.704897
-30.799892	-1.897316	1.316262	0.005818	0.704886
-30.661626	-1.919176	1.321267	0.005792	0.704891
-30.425044	-1.963640	1.326272	0.005748	0.704886
-30.746063	-1.905170	1.331277	0.005808	0.704889
-30.882213	-1.957464	1.336282	0.005834	0.704734
-31.541652	-1.913466	1.341286	0.005957	0.704586
-31.284193	-1.954911	1.346291	0.005909	0.704595
-31.765486	-1.870889	1.351296	0.005998	0.704591
-31.955259	-1.836398	1.356301	0.006034	0.704592
-31.091342	-1.987357	1.361306	0.005873	0.704598
-31.603709	-1.901514	1.366310	0.005969	0.704587
-31.704956	-1.944388	1.371315	0.005988	0.704464
-32.572311	-1.890005	1.376320	0.006149	0.704262
-32.154340	-1.963942	1.381325	0.006071	0.704263
-32.126886	-1.967985	1.386330	0.006066	0.704264
-32.475047	-1.908663	1.391334	0.006131	0.704259
-32.393956	-1.920256	1.396339	0.006116	0.704264
-32.735832	-1.861009	1.401344	0.006180	0.704261
-32.589077	-1.918570	1.406349	0.006153	0.704197
-32.990878	-1.965374	1.411354	0.006228	0.703958
-33.450475	-1.887923	1.416358	0.006313	0.703949
-33.556789	-1.864015	1.421363	0.006333	0.703959
-33.062215	-1.954398	1.426368	0.006241	0.703954
-33.306365	-1.911063	1.431373	0.006287	0.703954
-33.377811	-1.895268	1.436378	0.006300	0.703960
-33.176428	-1.951411	1.441382	0.006263	0.703919
-33.580114	-2.017209	1.446387	0.006338	0.703641
-34.079133	-1.930134	1.451392	0.006431	0.703637
-34.457606	-1.862385	1.456397	0.006501	0.703637
-33.684982	-1.996888	1.461402	0.006358	0.703644
-34.060703	-1.933034	1.466406	0.006428	0.703637
-34.255977	-1.895085	1.471411	0.006464	0.703643
-34.006783	-1.995945	1.476416	0.006418	0.703529
-35.238976	-1.867549	1.481421	0.006647	0.703345
-34.789227	-1.944993	1.486426	0.006564	0.703350
-34.911455	-1.927492	1.491430	0.006586	0.703341
-34.826226	-1.939247	1.496435	0.006571	0.703348
-34.809031	-1.942042	1.501440	0.006568	0.703348
-34.821871	-1.940256	1.506445	0.006570	0.703347
-34.607597	-2.092074	1.511450	0.006530	0.703118
-36.073923	-1.884853	1.516454	0.006803	0.703008
-35.869325	-1.918280	1.521459	0.006765	0.703014
-35.512898	-1.984343	1.526464	0.006699	0.703009
-35.656680	-1.959287	1.531469	0.006726	0.703008
-35.655250	-1.955214	1.536474	0.006726	0.703016
-35.804073	-1.943132	1.541478	0.006754	0.702987
-36.265178	-2.000929	1.546483	0.006839	0.702704
-36.593917	-1.944902	1.551488	0.006901	0.702698
-36.987909	-1.874459	1.556493	0.006974	0.702699
-36.591444	-1.942330	1.561498	0.006900	0.702704
-36.699727	-1.927890	1.566502	0.006921	0.702694
-36.812656	-1.903120	1.571507	0.006942	0.702703
-36.495836	-1.976412	1.576512	0.006883	0.702669
-37.254046	-1.987420	1.581517	0.007024	0.702374
-37.468197	-1.946417	1.586522	0.007064	0.702379
-37.868719	-1.879557	1.591526	0.007139	0.702370
-37.203388	-1.995835	1.596531	0.007015	0.702374
-37.537434	-1.937779	1.601536	0.007077	0.702371
-37.788492	-1.893091	1.606541	0.007124	0.702371
-37.273823	-2.006016	1.611546	0.007028	0.702328
-38.359762	-1.938366	1.616550	0.007231	0.702073
-38.516765	-1.905702	1.621555	0.007260	0.702082
-38.555394	-1.900165	1.626560	0.007267	0.702079
-38.352676	-1.938280	1.631565	0.007229	0.702075
-38.622166	-1.888374	1.636570	0.007280	0.702079
-38.654387	-1.886372	1.641574	0.007286	0.702071
-38.030894	-2.003221	1.646579	0.007170	0.702060
-38.804466	-2.018873	1.651584	0.007314	0.701749
-39.411456	-1.911140	1.656589	0.007427	0.701748
-39.236382	-1.940198	1.661594	0.007395	0.701752
-39.191186	-1.952500	1.666598	0.007386	0.701743
-39.342351	-1.921495	1.671603	0.007414	0.701751
-39.423003	-1.909197	1.676608	0.007429	0.701747
-39.433363	-1.925477	1.681613	0.007432	0.701710
-40.249506	-1.910669	1.686618	0.007584	0.701445
-40.544440	-1.860506	1.691622	0.007639	0.701440
-40.241878	-1.912916	1.696627	0.007582	0.701443
-40.144671	-1.931330	1.701632	0.007564	0.701441
-40.542212	-1.860672	1.706637	0.007638	0.701440
-40.253042	-1.909306	1.711642	0.007585	0.701446
-40.340926	-1.899341	1.716646	0.007601	0.701434
-40.554106	-1.937499	1.721651	0.007641	0.701280
-41.327283	-1.874509	1.726656	0.007785	0.701128
-40.773466	-1.974615	1.731661	0.007682	0.701125
-40.891671	-1.950839	1.736666	0.007704	0.701130
-41.626004	-1.823590	1.741670	0.007841	0.701123
-41.043121	-1.925682	1.746675	0.007732	0.701126
-40.875731	-1.956032	1.751680	0.007701	0.701125
-41.712137	-1.881863	1.756685	0.007857	0.700973
-42.035353	-1.868567	1.761690	0.007917	0.700883
-41.590605	-1.952383	1.766694	0.007835	0.700874
-41.599942	-1.945788	1.771699	0.007836	0.700884
-41.968347	-1.881093	1.776704	0.007905	0.700881
-41.923716	-1.890940	1.781709	0.007897	0.700877
-41.525153	-1.958739	1.786714	0.007823	0.700884
-42.605583	-1.929438	1.791718	0.008024	0.700553
-42.583453	-1.938505	1.796723	0.008020	0.700542
-42.629904	-1.930799	1.801728	0.008029	0.700541
-42.864370	-1.890296	1.806733	0.008072	0.700538
-42.488964	-1.953083	1.811738	0.008003	0.700546
-42.457179	-1.964296	1.816742	0.007997	0.700535
-42.583688	-2.006297	1.821747	0.008020	0.700404
-43.674196	-1.900887	1.826752	0.008223	0.700223
-43.111370	-2.004106	1.831757	0.008119	0.700217
-43.187205	-1.984347	1.836762	0.008133	0.700230
-43.954429	-1.851682	1.841766	0.008276	0.700221
-43.404848	-1.946843	1.846771	0.008174	0.700227
-43.318242	-1.963865	1.851776	0.008158	0.700223
-44.274443	-1.941085	1.856781	0.008336	0.699923
-44.449793	-1.919315	1.861786	0.008368	0.699904
-44.639457	-1.887222	1.866790	0.008404	0.699900
-44.373565	-1.933601	1.871795	0.008354	0.699902
-44.723644	-1.872631	1.876800	0.008420	0.699899
-44.677185	-1.882724	1.881805	0.008411	0.699895
-44.242644	-1.956641	1.886810	0.008330	0.699902
-44.901478	-1.943831	1.891814	0.008453	0.699690
-45.401291	-1.898566	1.896819	0.008546	0.699601
-45.084153	-1.953203	1.901824	0.008487	0.699604
-45.274018	-1.921764	1.906829	0.008523	0.699599
-45.342697	-1.906632	1.911834	0.008536	0.699605
-45.369080	-1.906425	1.916838	0.008541	0.699596
-45.133611	-1.945304	1.921843	0.008497	0.699602
-45.926088	-1.949849	1.926848	0.008644	0.699305
-46.199748	-1.920220	1.931853	0.008695	0.699266
-45.891196	-1.971290	1.936858	0.008638	0.699274
-46.288527	-1.905424	1.941862	0.008712	0.699264
-46.228783	-1.912812	1.946867	0.008701	0.699270
-45.769550	-1.995751	1.951872	0.008616	0.699268
-46.019291	-1.990445	1.956877	0.008662	0.699188
-47.056001	-1.915002	1.961882	0.008855	0.698966
-46.919727	-1.942034	1.966886	0.008830	0.698960
-46.932013	-1.938536	1.971891	0.008832	0.698963
-46.880721	-1.948567	1.976896	0.008823	0.698961
-47.083197	-1.916258	1.981901	0.008861	0.698953
-46.751470	-1.971772	1.986906	0.008799	0.698960
-47.094563	-1.979215	1.991910	0.008863	0.698820
-48.104520	-1.888209	1.996915	0.009051	0.698639
-47.730009	-1.954380	2.001920	0.008982	0.698640
-47.773139	-1.946226	2.011917	0.008990	0.698641
-47.792777	-1.942262	2.021914	0.008994	0.698641
-47.466235	-2.001463	2.031910	0.008933	0.698639
-48.169937	-1.927386	2.041907	0.009064	0.698534
-48.173025	-1.962002	2.051904	0.009065	0.698462
-48.501989	-1.894260	2.061901	0.009126	0.698481
-47.676105	-1.996013	2.071898	0.008973	0.698573
-47.819996	-1.936177	2.081894	0.009000	0.698642
-47.768887	-1.945176	2.091891	0.008990	0.698642
-47.560735	-1.982032	2.101888	0.008952	0.698642
-47.885720	-1.925030	2.111885	0.009012	0.698640
-47.853189	-1.930409	2.121882	0.009006	0.698641
-47.902371	-1.920753	2.131878	0.009016	0.698642
-47.887199	-1.924382	2.141875	0.009013	0.698640
-47.167885	-1.923867	2.151872	0.008879	0.698901
-47.055895	-1.915073	2.161869	0.008859	0.698959
-46.760435	-1.967576	2.171866	0.008804	0.698960
-47.032373	-1.919768	2.181862	0.008854	0.698958
-47.071561	-1.878163	2.191859	0.008862	0.699028
-45.991959	-1.952639	2.201856	0.008661	0.699267
-45.958968	-1.958561	2.211853	0.008655	0.699267
-45.925538	-1.962138	2.221850	0.008649	0.699271
-45.988150	-1.937619	2.231846	0.008661	0.699298
-45.322032	-1.909969	2.241843	0.008537	0.699595
-44.961792	-1.973714	2.251840	0.008470	0.699596
-45.214432	-1.929043	2.261837	0.008517	0.699595
-45.002212	-1.934667	2.271834	0.008478	0.699660
-44.225763	-1.957578	2.281830	0.008334	0.699894
-44.109179	-1.979563	2.291827	0.008312	0.699892
-44.360378	-1.934649	2.301824	0.008359	0.699891
-44.160122	-1.905961	2.311821	0.008322	0.700022
-43.287181	-1.965473	2.321818	0.008159	0.700217
-43.471119	-1.932401	2.331814	0.008194	0.700217
-43.533936	-1.922471	2.341811	0.008206	0.700214
-42.724594	-1.922352	2.351808	0.008055	0.700507
-42.493443	-1.949810	2.361805	0.008012	0.700534
-42.458811	-1.955910	2.371802	0.008006	0.700534
-42.567837	-1.891051	2.381798	0.008026	0.700626
-41.736793	-1.919473	2.391795	0.007872	0.700868
-41.594787	-1.942636	2.401792	0.007846	0.700872
-41.702864	-1.923904	2.411789	0.007866	0.700871
-40.897959	-1.967757	2.421786	0.007716	0.701072
-40.990083	-1.926019	2.431782	0.007733	0.701123
-40.765340	-1.968218	2.441779	0.007692	0.701119
-40.856595	-1.897615	2.451776	0.007709	0.701228
-39.838448	-1.975654	2.461773	0.007520	0.701438
-39.892336	-1.964926	2.471770	0.007530	0.701440
-40.163780	-1.917874	2.481766	0.007580	0.701437
-39.343110	-1.923863	2.491763	0.007428	0.701720
-39.371620	-1.906962	2.501760	0.007433	0.701744
-39.308114	-1.917591	2.511757	0.007422	0.701745
-38.720644	-1.912838	2.521754	0.007312	0.701966
-38.417797	-1.912594	2.531750	0.007256	0.702076
-38.215992	-1.949699	2.541747	0.007219	0.702073
-38.355171	-1.890879	2.551744	0.007245	0.702142
-37.347533	-1.955140	2.561741	0.007057	0.702375
-37.480843	-1.932415	2.571738	0.007082	0.702372
-37.647320	-1.903311	2.581734	0.007113	0.702371
-37.019942	-1.875714	2.591731	0.006997	0.702652
-36.751525	-1.903541	2.601728	0.006947	0.702693
-36.667304	-1.917437	2.611725	0.006931	0.702694
-36.439142	-1.871437	2.621722	0.006889	0.702869
-35.883730	-1.901485	2.631718	0.006786	0.703008
-35.828036	-1.912500	2.641715	0.006776	0.703006
-35.838725	-1.872054	2.651712	0.006778	0.703083
-34.528734	-1.977895	2.661709	0.006534	0.703341
-34.946871	-1.900673	2.671706	0.006612	0.703346
-34.800771	-1.928001	2.681702	0.006585	0.703343
-34.456465	-1.897550	2.691699	0.006521	0.703528
-33.885422	-1.947277	2.701696	0.006415	0.703633
-33.929573	-1.938864	2.711693	0.006423	0.703634
-33.833759	-1.954321	2.721690	0.006406	0.703637
-33.242345	-1.906012	2.731686	0.006296	0.703947
-33.094089	-1.929268	2.741683	0.006268	0.703953
-33.211068	-1.909885	2.751680	0.006290	0.703949
-32.721581	-1.908760	2.761677	0.006199	0.704127
-32.274681	-1.921844	2.771674	0.006116	0.704261
-32.259860	-1.923402	2.781670	0.006113	0.704263
-32.369362	-1.883916	2.791667	0.006134	0.704303
-31.557150	-1.886645	2.801664	0.005983	0.704589
-31.303861	-1.932423	2.811661	0.005936	0.704588
-31.405154	-1.911263	2.821658	0.005955	0.704594
-30.922441	-1.895069	2.831654	0.005865	0.704799
-30.690172	-1.891705	2.841651	0.005822	0.704889
-30.788832	-1.874001	2.851648	0.005841	0.704889
-30.414559	-1.874601	2.861645	0.005771	0.705022
-29.653866	-1.913410	2.871642	0.005630	0.705216
-29.528188	-1.934962	2.881638	0.005606	0.705218
-29.704230	-1.905676	2.891635	0.005639	0.705213
-29.035059	-1.893849	2.901632	0.005515	0.705477
-28.868221	-1.897494	2.911629	0.005484	0.705529
-28.585127	-1.946564	2.921626	0.005432	0.705532
-28.489587	-1.932369	2.931622	0.005414	0.705594
-27.871856	-1.907758	2.941619	0.005299	0.705865
-27.777271	-1.924115	2.951616	0.005282	0.705866
-27.702622	-1.937113	2.961613	0.005268	0.705866
-27.488158	-1.906521	2.971610	0.005228	0.706004
-26.898312	-1.947146	2.981606	0.005118	0.706133
-27.254910	-1.883697	2.991603	0.005185	0.706133
-27.125741	-1.877762	3.001600	0.005161	0.706191
-26.430319	-1.873489	3.011597	0.005032	0.706448
-26.165274	-1.920270	3.021594	0.004983	0.706449
-26.162952	-1.920258	3.031590	0.004982	0.706449
-25.895849	-1.831102	3.041587	0.004933	0.706724
-25.238383	-1.931879	3.051584	0.004810	0.706756
-25.333040	-1.915047	3.061581	0.004828	0.706756
-25.007108	-1.885278	3.071578	0.004768	0.706932
-24.254998	-1.942741	3.081574	0.004628	0.707086
-24.693901	-1.863614	3.091571	0.004710	0.707087
-24.414117	-1.905857	3.101568	0.004658	0.707102
-23.624876	-1.907298	3.111565	0.004511	0.707381
-23.429798	-1.940203	3.121562	0.004475	0.707385
-23.566667	-1.916237	3.131558	0.004500	0.707384
-23.390651	-1.862818	3.141555	0.004468	0.707553
-22.398234	-1.964323	3.151552	0.004283	0.707704
-22.781257	-1.895392	3.161549	0.004355	0.707705
-22.677409	-1.912657	3.171546	0.004336	0.707708
-21.883558	-1.907500	3.181542	0.004188	0.708001
-21.970650	-1.884027	3.191539	0.004204	0.708017
-21.854310	-1.905974	3.201536	0.004183	0.708014
-21.543955	-1.878368	3.211533	0.004125	0.708180
-20.749251	-1.932193	3.221530	0.003977	0.708356
-21.090960	-1.872032	3.231526	0.004041	0.708354
-20.917231	-1.904169	3.241523	0.004009	0.708351
-20.148269	-1.897591	3.251520	0.003866	0.708639
-20.243116	-1.879791	3.261517	0.003884	0.708640
-19.881385	-1.944381	3.271514	0.003817	0.708640
-19.879360	-1.858309	3.281510	0.003816	0.708813
-19.379604	-1.874001	3.291507	0.003723	0.708959
-19.297729	-1.889181	3.301504	0.003708	0.708958
-19.362200	-1.845994	3.311501	0.003720	0.709021
-18.133747	-1.941664	3.321498	0.003492	0.709267
-18.378626	-1.897984	3.331494	0.003538	0.709267
-18.282361	-1.915572	3.341491	0.003520	0.709266
-17.771055	-1.899714	3.351488	0.003425	0.709480
-17.339706	-1.916892	3.361485	0.003345	0.709599
-17.289243	-1.924794	3.371482	0.003335	0.709601
-17.291848	-1.925270	3.381478	0.003336	0.709598
-16.682771	-1.899341	3.391475	0.003223	0.709867
-16.654416	-1.891263	3.401472	0.003218	0.709893
-16.476440	-1.921498	3.411469	0.003185	0.709896
-16.317109	-1.874091	3.421466	0.003155	0.710047
-15.421600	-1.947458	3.431462	0.002989	0.710219
-15.490011	-1.935582	3.441459	0.003002	0.710218
-15.539148	-1.925615	3.451456	0.003011	0.710220
-14.986761	-1.915786	3.461453	0.002908	0.710436
-14.586176	-1.936392	3.471450	0.002834	0.710537
-14.906736	-1.879191	3.481446	0.002894	0.710537
-14.614338	-1.907158	3.491443	0.002839	0.710585
-14.026199	-1.868018	3.501440	0.002730	0.710872
-13.604450	-1.942394	3.511437	0.002652	0.710873
-13.695037	-1.924688	3.521434	0.002669	0.710876
-13.436553	-1.890257	3.531430	0.002621	0.711036
-12.993892	-1.916668	3.541427	0.002538	0.711141
-13.090685	-1.900402	3.551424	0.002557	0.711138
-12.998879	-1.882653	3.561421	0.002540	0.711206
-11.883798	-1.954632	3.571418	0.002332	0.711459
-11.998091	-1.934778	3.581414	0.002354	0.711457
-11.736547	-1.982249	3.591411	0.002305	0.711455
-11.954902	-1.865325	3.601408	0.002346	0.711611
-10.984092	-1.962595	3.611405	0.002165	0.711761
-11.168966	-1.928597	3.621402	0.002200	0.711763
-10.916590	-1.974316	3.631398	0.002153	0.711761
-10.245308	-1.943849	3.641395	0.002028	0.712060
-10.218443	-1.933384	3.651392	0.002023	0.712090
-9.835782	-2.001415	3.661389	0.001952	0.712090
-10.102724	-1.935577	3.671386	0.002002	0.712126
-9.420285	-1.925731	3.681382	0.001875	0.712388
-9.227524	-1.961297	3.691379	0.001840	0.712385
-9.349147	-1.939432	3.701376	0.001862	0.712385
-8.779689	-1.950338	3.711373	0.001756	0.712565
-8.220362	-1.977116	3.721370	0.001652	0.712710
-8.175095	-1.984439	3.731366	0.001644	0.712711
-8.474656	-1.931930	3.741363	0.001700	0.712709
-7.807585	-1.909450	3.751360	0.001576	0.712990
-7.395489	-1.966346	3.761357	0.001500	0.713023
-7.297876	-1.981856	3.771354	0.001482	0.713026
-7.258715	-1.950192	3.781350	0.001474	0.713103
-6.409358	-1.971538	3.791347	0.001316	0.713361
-6.513657	-1.953195	3.801344	0.001336	0.713360
-6.578226	-1.941419	3.811341	0.001348	0.713361
-6.214941	-1.910108	3.821338	0.001281	0.713551
-5.454872	-1.992863	3.831334	0.001139	0.713656
-5.682878	-1.951811	3.841331	0.001182	0.713656
-5.761932	-1.919648	3.851328	0.001197	0.713692
-4.573408	-1.991196	3.861325	0.000976	0.713970
-4.741506	-1.960740	3.871322	0.001007	0.713971
-4.570671	-1.989725	3.881318	0.000975	0.713974
-4.635970	-1.903170	3.891315	0.000988	0.714122
-3.658686	-1.998962	3.901312	0.000806	0.714277
-3.731586	-1.985230	3.911309	0.000820	0.714279
-3.768831	-1.977143	3.921306	0.000827	0.714281
-3.248004	-1.944169	3.931302	0.000730	0.714531
-2.962325	-1.955196	3.941299	0.000677	0.714610
-2.890735	-1.968741	3.951296	0.000664	0.714608
-2.726069	-1.969856	3.961293	0.000633	0.714663
-2.303486	-1.922616	3.971290	0.000555	0.714906
-2.294465	-1.922297	3.981286	0.000553	0.714910
-2.120164	-1.955361	3.991283	0.000521	0.714905
-2.103960	-1.813541	4.001280	0.000518	0.715192
-1.372467	-1.923174	4.011277	0.000382	0.715233
-1.696937	-1.865690	4.021274	0.000443	0.715232
-1.469394	-1.762397	4.031270	0.000400	0.715517
-1.175005	-1.798605	4.041267	0.000346	0.715549
-1.725775	-1.645031	4.051264	0.000448	0.715659
-0.905135	-1.676842	4.061261	0.000296	0.715885
-1.243913	-1.615076	4.071258	0.000359	0.715887
-0.912598	-1.549740	4.081254	0.000297	0.716134
-0.722907	-1.584206	4.091251	0.000262	0.716132
-0.976857	-1.404901	4.101248	0.000309	0.716397
-0.592592	-1.447506	4.111245	0.000238	0.716448
-0.598628	-1.303104	4.121242	0.000239	0.716731
-0.637644	-1.261373	4.131238	0.000247	0.716800
-0.681347	-1.110152	4.141235	0.000255	0.717084
-0.605904	-1.041818	4.151232	0.000241	0.717245
-0.620769	-0.965875	4.161229	0.000244	0.717390
-0.643029	-0.802898	4.171226	0.000248	0.717704
-0.560750	-0.717757	4.181222	0.000233	0.717901
-0.367386	-0.640901	4.191219	0.000197	0.718120
-0.273109	-0.541732	4.201216	0.000179	0.718349
-0.186112	-0.410511	4.211213	0.000163	0.718638
-0.333132	-0.265747	4.221210	0.000191	0.718872
-0.158309	-0.169194	4.231206	0.000158	0.719124
-0.100535	-0.042596	4.241203	0.000148	0.719393
-0.206643	0.120614	4.251200	0.000167	0.719678
0.000000	0.260365	4.261197	0.000129	0.720025
-0.100089	0.887588	4.266202	0.000147	0.721225
0.271626	2.082586	4.271206	0.000077	0.723701
0.401860	3.910955	4.276211	0.000052	0.727322
0.669100	6.273363	4.281216	0.000001	0.732007
0.974890	9.136541	4.286221	-0.000058	0.737640
1.094465	12.499551	4.291226	-0.000082	0.744120
1.808034	16.228544	4.296230	-0.000217	0.751434
1.974845	20.452129	4.301235	-0.000251	0.759421
2.482722	25.010736	4.306240	-0.000349	0.768056
3.101477	29.930549	4.311245	-0.000467	0.777290
3.402774	35.237401	4.316250	-0.000526	0.787011
3.833092	40.859547	4.321254	-0.000610	0.797216
4.294115	46.760602	4.326259	-0.000700	0.807791
4.752293	52.955027	4.331264	-0.000789	0.818736
5.448092	59.381624	4.336269	-0.000923	0.830006
5.717017	66.107257	4.341274	-0.000977	0.841501
6.226426	73.016687	4.346278	-0.001076	0.853218
8.887568	79.743653	4.351283	-0.001576	0.865097
13.139751	86.465214	4.356288	-0.002372	0.877259
13.658334	94.040227	4.361293	-0.002474	0.889565
14.315843	101.733387	4.366298	-0.002601	0.901928
15.093097	109.563245	4.371302	-0.002751	0.914368
16.056000	117.455573	4.376307	-0.002935	0.926786
16.952991	125.494925	4.381312	-0.003107	0.939243
17.544287	133.688456	4.386317	-0.003223	0.951687
18.726227	141.854350	4.391322	-0.003448	0.964081
19.624048	150.178508	4.396326	-0.003620	0.976475
20.751604	158.532224	4.401331	-0.003836	0.988813
21.676718	166.985349	4.406336	-0.004013	1.001089
22.375193	175.504775	4.411341	-0.004149	1.013253
23.644247	183.955723	4.416346	-0.004391	1.025315
24.665454	192.502999	4.421350	-0.004586	1.037309
25.775946	201.042569	4.426355	-0.004799	1.049175
26.652702	209.661968	4.431360	-0.004967	1.060961
27.400536	218.338453	4.436365	-0.005112	1.072663
28.052249	227.007378	4.441370	-0.005239	1.084207
28.951677	235.665833	4.446374	-0.005412	1.095670
29.618662	244.342546	4.451379	-0.005542	1.106986
30.221502	253.045121	4.456384	-0.005660	1.118206
30.726908	261.740702	4.461389	-0.005759	1.129285
31.062858	270.456774	4.466394	-0.005828	1.140245
32.526499	279.009813	4.471398	-0.006106	1.151138
33.237874	287.661318	4.476403	-0.006244	1.161890
33.924526	296.302854	4.481408	-0.006377	1.172527
34.868419	304.893981	4.486413	-0.006558	1.183060
35.346549	313.554293	4.491418	-0.006653	1.193487
35.902336	322.178214	4.496422	-0.006762	1.203797
36.902687	330.714092	4.501427	-0.006954	1.214004
37.587184	339.291309	4.506432	-0.007087	1.224111
38.005486	347.932141	4.511437	-0.007170	1.234156
38.833968	356.428004	4.516442	-0.007330	1.244034
39.888174	364.919539	4.521446	-0.007532	1.253872
40.689516	373.418773	4.526451	-0.007686	1.263594
41.481004	381.930394	4.531456	-0.007839	1.273253
42.276191	390.421794	4.536461	-0.007993	1.282817
42.716757	398.952642	4.541466	-0.008080	1.292288
43.805468	407.371426	4.546470	-0.008288	1.301687
44.275587	415.941336	4.551475	-0.008381	1.311068
45.019710	424.436421	4.556480	-0.008525	1.320352
45.810014	432.839914	4.561485	-0.008678	1.329481
46.270839	441.287187	4.566490	-0.008769	1.338536
47.056966	449.679906	4.571494	-0.008921	1.347529
47.705745	458.092211	4.576499	-0.009047	1.356459
47.943074	466.531419	4.581504	-0.009097	1.365287
48.778871	474.896453	4.586509	-0.009258	1.374084
49.105587	483.303591	4.591514	-0.009324	1.382782
49.954001	491.647287	4.596518	-0.009487	1.391448
50.534502	499.996694	4.601523	-0.009601	1.400022
51.195839	508.319502	4.606528	-0.009729	1.408529
51.923779	516.655339	4.611533	-0.009870	1.417009
52.472288	524.984095	4.616538	-0.009978	1.425402
53.178673	533.322063	4.621542	-0.010114	1.433781
53.761174	541.632101	4.626547	-0.010228	1.442063
54.414715	549.939637	4.631552	-0.010355	1.450307
54.935721	558.273494	4.636557	-0.010458	1.458508
55.370137	566.591050	4.641562	-0.010544	1.466633
56.128336	574.925048	4.646566	-0.010690	1.474780
56.706080	583.196564	4.651571	-0.010803	1.482795
57.212167	591.477750	4.656576	-0.010903	1.490764
57.480052	599.805910	4.661581	-0.010958	1.498698
57.584638	608.122268	4.666586	-0.010983	1.506554
58.258746	616.374898	4.671590	-0.011114	1.514396
58.511961	624.651349	4.676595	-0.011166	1.522157
59.232500	632.866285	4.681600	-0.011306	1.529891
59.638606	641.151769	4.686605	-0.011386	1.537604
60.089389	649.380391	4.691610	-0.011476	1.545232
60.569580	657.666064	4.696614	-0.011570	1.552880
60.881855	665.909819	4.701619	-0.011634	1.560427
61.307150	674.139546	4.706624	-0.011718	1.567942
61.865391	682.372412	4.711629	-0.011828	1.575442
62.564635	690.545920	4.716634	-0.011963	1.582874
63.569828	698.699647	4.721638	-0.012155	1.590298
64.074802	706.938613	4.726643	-0.012255	1.597690
64.538808	715.153260	4.731648	-0.012346	1.605022
65.062307	723.389759	4.736653	-0.012449	1.612347
65.360446	731.622814	4.741658	-0.012510	1.619604
65.784204	739.854622	4.746662	-0.012594	1.626846
66.168480	748.127963	4.751667	-0.012671	1.634085
67.000665	756.252845	4.756672	-0.012831	1.641226
67.578731	764.440775	4.761677	-0.012944	1.648356
68.201226	772.617436	4.766682	-0.013065	1.655450
68.553786	780.841115	4.771686	-0.013136	1.662518
68.995305	789.032171	4.776691	-0.013224	1.669540
69.615061	797.200029	4.781696	-0.013344	1.676537
70.336669	805.352992	4.786701	-0.013484	1.683505
70.715047	813.546765	4.791706	-0.013560	1.690434
71.251868	821.747506	4.796710	-0.013665	1.697360
71.548529	829.950172	4.801715	-0.013725	1.704228
72.149426	838.124376	4.806720	-0.013842	1.711085
72.673073	846.324118	4.811725	-0.013945	1.717925
73.020561	854.477387	4.816730	-0.014015	1.724677
73.617669	862.654352	4.821734	-0.014132	1.731454
73.823229	870.863308	4.826739	-0.014175	1.738180
74.374315	878.998647	4.831744	-0.014283	1.744865
75.142483	887.136843	4.836749	-0.014431	1.751553
75.452968	895.304396	4.841754	-0.014494	1.758182
75.971065	903.456138	4.846758	-0.014596	1.764800
76.395408	911.627656	4.851763	-0.014680	1.771396
76.783512	919.797109	4.856768	-0.014758	1.777962
77.412960	927.920515	4.861773	-0.014880	1.784497
77.470714	936.159916	4.866778	-0.014896	1.791029
78.032521	944.317663	4.871782	-0.015006	1.797534
78.152464	952.487619	4.876787	-0.015034	1.803972
78.758090	960.581274	4.881792	-0.015152	1.810386
79.280220	968.720336	4.886797	-0.015254	1.816803
79.617569	976.853267	4.891802	-0.015322	1.823170
80.009802	985.014593	4.896806	-0.015400	1.829543
80.479515	993.142653	4.901811	-0.015493	1.835877
81.115614	1001.236926	4.906816	-0.015617	1.842183
81.517598	1009.383446	4.911821	-0.015697	1.848480
81.958106	1017.534245	4.916826	-0.015784	1.854763
82.638660	1025.633288	4.921830	-0.015916	1.861014
83.024183	1033.780385	4.926835	-0.015993	1.867245
83.361457	1041.957070	4.931840	-0.016061	1.873473
83.758980	1050.094697	4.936845	-0.016140	1.879657
84.207995	1058.193233	4.941850	-0.016229	1.885797
84.635633	1066.336239	4.946854	-0.016314	1.891948
85.062478	1074.458971	4.951859	-0.016399	1.898064
85.395483	1082.592298	4.956864	-0.016466	1.904158
85.818098	1090.740744	4.961869	-0.016550	1.910253
85.953577	1098.897757	4.966874	-0.016580	1.916302
86.521670	1106.979304	4.971878	-0.016691	1.922326
86.995845	1115.082597	4.976883	-0.016785	1.928336
87.486441	1123.209772	4.981888	-0.016881	1.934346
88.130559	1131.303196	4.986893	-0.017006	1.940330
88.256331	1139.448983	4.991898	-0.017035	1.946276
88.657017	1147.612795	4.996902	-0.017115	1.952248
89.026681	1155.725199	5.001907	-0.017189	1.958160
89.401278	1163.824247	5.006912	-0.017264	1.964046
89.690239	1171.947475	5.011917	-0.017323	1.969922
90.076032	1180.040237	5.016922	-0.017400	1.975769
90.771430	1188.104605	5.021926	-0.017534	1.981611
91.267454	1196.207934	5.026931	-0.017632	1.987443
91.667805	1204.325540	5.031936	-0.017712	1.993258
92.156379	1212.435361	5.036941	-0.017808	1.999059
92.601504	1220.514797	5.041946	-0.017896	2.004817
92.873964	1228.663377	5.046950	-0.017952	2.010589
93.112489	1236.791708	5.051955	-0.018002	2.016327
93.629103	1244.857952	5.056960	-0.018103	2.022034
93.958106	1252.997015	5.061965	-0.018169	2.027756
94.117459	1261.147786	5.066970	-0.018204	2.033453
94.733797	1269.210476	5.071974	-0.018324	2.039119
95.157107	1277.276648	5.076979	-0.018408	2.044752
95.499091	1285.378258	5.081984	-0.018477	2.050386
96.007557	1293.482359	5.086989	-0.018577	2.056023
96.170628	1301.596440	5.091994	-0.018613	2.061616
96.582056	1309.692765	5.096998	-0.018694	2.067207
97.007699	1317.799446	5.102003	-0.018779	2.072791
97.252851	1325.909479	5.107008	-0.018830	2.078345
97.680015	1333.993315	5.112013	-0.018914	2.083883
98.000836	1342.084271	5.117018	-0.018979	2.089402
98.279465	1350.215951	5.122022	-0.019036	2.094929
98.690692	1358.287325	5.127027	-0.019118	2.100414
99.183498	1366.359496	5.132032	-0.019215	2.105892
99.601715	1374.512784	5.137037	-0.019298	2.111404
100.253065	1382.579799	5.142042	-0.019425	2.116866
100.779842	1390.633674	5.147046	-0.019528	2.122293
101.005903	1398.720887	5.152051	-0.019575	2.127699
101.531531	1406.777555	5.157056	-0.019678	2.133100
101.904404	1414.886189	5.162061	-0.019753	2.138507
102.046971	1422.990237	5.167066	-0.019785	2.143876
102.302716	1431.105159	5.172070	-0.019838	2.149248
102.484266	1439.231471	5.177075	-0.019877	2.154608
102.873638	1447.282011	5.182080	-0.019954	2.159925
103.127339	1455.355789	5.187085	-0.020007	2.165230
103.488881	1463.431106	5.192090	-0.020079	2.170534
103.724926	1471.541662	5.197094	-0.020128	2.175836
104.065850	1479.620719	5.202099	-0.020197	2.181114
104.425274	1487.679597	5.207104	-0.020269	2.186368
104.904114	1495.804830	5.212109	-0.020363	2.191663
105.121844	1503.893675	5.217114	-0.020409	2.196898
105.623653	1511.931259	5.222118	-0.020508	2.202113
106.094153	1520.002677	5.227123	-0.020601	2.207335
106.341192	1528.101349	5.232128	-0.020652	2.212542
106.723241	1536.181954	5.237133	-0.020728	2.217737
107.115574	1544.220991	5.242138	-0.020806	2.222894
107.603992	1552.300678	5.247142	-0.020902	2.228073
108.026243	1560.399679	5.252147	-0.020986	2.233247
108.539067	1568.443116	5.257152	-0.021087	2.238381
109.059933	1576.507496	5.262157	-0.021189	2.243518
109.273643	1584.601561	5.267162	-0.021234	2.248634
109.577570	1592.726784	5.272166	-0.021296	2.253766
110.136678	1600.761242	5.277171	-0.021405	2.258852
110.306513	1608.857271	5.282176	-0.021442	2.263931
110.540953	1616.975677	5.287181	-0.021491	2.269018
110.540618	1625.157283	5.292186	-0.021496	2.274112
111.199628	1633.146365	5.297190	-0.021624	2.279133
111.597260	1641.191134	5.302195	-0.021703	2.284154
111.943715	1649.252107	5.307200	-0.021773	2.289170
112.455999	1657.333756	5.312205	-0.021873	2.294201
112.664592	1665.391276	5.317210	-0.021917	2.299181
112.888399	1673.469164	5.322214	-0.021964	2.304164
113.186342	1681.541290	5.327219	-0.022025	2.309139
113.562404	1689.618305	5.332224	-0.022100	2.314112
113.939731	1697.672867	5.337229	-0.022175	2.319061
114.386944	1705.700482	5.342234	-0.022264	2.323989
115.139706	1713.737995	5.347238	-0.022409	2.328938
115.263461	1721.861222	5.352243	-0.022437	2.333876
115.499858	1729.931199	5.357248	-0.022487	2.338781
116.153195	1737.984471	5.362253	-0.022613	2.343699
116.307757	1746.067231	5.367258	-0.022647	2.348584
116.814306	1754.168661	5.372262	-0.022747	2.353499
117.014648	1762.236865	5.377267	-0.022789	2.358358
117.287257	1770.277153	5.382272	-0.022845	2.363197
117.504610	1778.372662	5.387277	-0.022891	2.368054
117.791154	1786.440020	5.392282	-0.022950	2.372890
118.577264	1794.455880	5.397286	-0.023101	2.377726
118.781370	1802.541413	5.402291	-0.023144	2.382546
118.920846	1810.622874	5.407296	-0.023175	2.387349
119.376120	1818.699601	5.412301	-0.023265	2.392165
119.742540	1826.747101	5.417306	-0.023339	2.396946
119.862674	1834.826799	5.422310	-0.023366	2.401718
120.337112	1842.866179	5.427315	-0.023460	2.406484
120.523979	1850.955530	5.432320	-0.023500	2.411247
120.814782	1859.031743	5.437325	-0.023559	2.416001
121.109570	1867.077039	5.442330	-0.023619	2.420729
121.572584	1875.124296	5.447334	-0.023711	2.425461
121.917499	1883.208020	5.452339	-0.023780	2.430195
121.934343	1891.374697	5.457344	-0.023788	2.434944
122.308414	1899.392030	5.462349	-0.023863	2.439624
122.536113	1907.421064	5.467354	-0.023911	2.444291
122.918724	1915.483364	5.472358	-0.023987	2.448979
123.330459	1923.540485	5.477363	-0.024069	2.453658
123.670905	1931.591389	5.482368	-0.024137	2.458319
124.163622	1939.625102	5.487373	-0.024234	2.462972
124.256522	1947.686509	5.492378	-0.024257	2.467603
124.730497	1955.749730	5.497382	-0.024350	2.472254
125.018510	1963.818209	5.502387	-0.024409	2.476886
125.450404	1971.834511	5.507392	-0.024495	2.481490
125.955755	1979.866601	5.512397	-0.024594	2.486099
126.319849	1987.919866	5.517402	-0.024667	2.490702
126.754539	1996.013016	5.522406	-0.024753	2.495324
127.146212	2004.053597	5.527411	-0.024831	2.499904
127.678034	2012.063996	5.532416	-0.024935	2.504469
127.986723	2020.176002	5.537421	-0.024998	2.509067
128.171317	2028.289915	5.542426	-0.025037	2.513648
128.609915	2036.321902	5.547430	-0.025124	2.518193
128.886907	2044.372976	5.552435	-0.025181	2.522729
128.905564	2052.437204	5.557440	-0.025190	2.527246
129.221041	2060.514826	5.562445	-0.025254	2.531783
129.639437	2068.551436	5.567450	-0.025337	2.536296
129.856334	2076.616534	5.572454	-0.025382	2.540803
130.077880	2084.663183	5.577459	-0.025429	2.545292
130.457477	2092.699592	5.582464	-0.025505	2.549779
130.656782	2100.802045	5.587469	-0.025547	2.554281
130.774966	2108.851222	5.592474	-0.025574	2.558740
131.116698	2116.871527	5.597478	-0.025643	2.563192
131.468858	2124.917432	5.602483	-0.025713	2.567650
131.707103	2132.983675	5.607488	-0.025763	2.572104
132.240569	2141.033140	5.612493	-0.025868	2.576561
132.952093	2149.022623	5.617498	-0.026005	2.580989
133.430454	2157.063816	5.622502	-0.026099	2.585423
133.682650	2165.159751	5.627507	-0.026152	2.589863
133.815950	2173.415258	5.632512	-0.026182	2.594374
134.284975	2181.414270	5.637517	-0.026274	2.598760
134.592076	2189.399854	5.642522	-0.026336	2.603121
135.084527	2197.401276	5.647526	-0.026433	2.607496
135.447769	2205.458465	5.652531	-0.026506	2.611884
135.531532	2213.529170	5.657536	-0.026527	2.616254
135.798267	2221.569330	5.662541	-0.026582	2.620612
136.047500	2229.594770	5.667546	-0.026633	2.624954
136.359635	2237.654048	5.672550	-0.026697	2.629311
136.441079	2245.751276	5.677555	-0.026717	2.633666
136.795117	2253.762255	5.682560	-0.026788	2.637985
137.186109	2261.798963	5.687565	-0.026866	2.642313
137.330278	2269.838180	5.692570	-0.026898	2.646619
137.842758	2277.877053	5.697574	-0.026998	2.650943
138.091107	2285.949079	5.702579	-0.027050	2.655259
138.348039	2293.968138	5.707584	-0.027103	2.659541
138.622699	2302.026949	5.712589	-0.027159	2.663838
139.044256	2310.069852	5.717594	-0.027243	2.668129
139.084402	2318.173523	5.722598	-0.027256	2.672421
139.507175	2326.217191	5.727603	-0.027339	2.676699
139.796780	2334.223796	5.732608	-0.027398	2.680942
140.152191	2342.257838	5.737613	-0.027470	2.685196
140.147659	2350.315653	5.742618	-0.027474	2.689434
140.493654	2358.401616	5.747622	-0.027544	2.693702
141.000576	2366.411502	5.752627	-0.027643	2.697933
141.227192	2374.454239	5.757632	-0.027691	2.702157
141.491943	2382.503329	5.762637	-0.027745	2.706380
141.995428	2390.537140	5.767642	-0.027844	2.710604
142.245494	2398.609304	5.772646	-0.027896	2.714824
142.564857	2406.650467	5.777651	-0.027960	2.719027
142.772752	2414.679054	5.782656	-0.028004	2.723210
143.157308	2422.739446	5.787661	-0.028081	2.727413
143.284701	2430.803847	5.792666	-0.028110	2.731596
143.539886	2438.850415	5.797670	-0.028163	2.735772
143.896534	2446.886514	5.802675	-0.028234	2.739941
144.254301	2454.894922	5.807680	-0.028306	2.744090
144.676150	2462.948168	5.812685	-0.028390	2.748260
145.150535	2471.036280	5.817690	-0.028483	2.752445
145.403009	2479.135083	5.822694	-0.028535	2.756615
145.797631	2487.126520	5.827699	-0.028614	2.760732
145.801594	2495.141125	5.832704	-0.028620	2.764831
146.230723	2503.187584	5.837709	-0.028705	2.768967
146.422758	2511.248923	5.842714	-0.028746	2.773089
146.752689	2519.283575	5.847718	-0.028812	2.777200
146.949053	2527.335442	5.852723	-0.028854	2.781305
147.267467	2535.356202	5.857728	-0.028919	2.785396
147.562312	2543.418796	5.862733	-0.028979	2.789500
147.918883	2551.469616	5.867738	-0.029050	2.793596
148.112076	2559.499447	5.872742	-0.029091	2.797666
148.426302	2567.541338	5.877747	-0.029155	2.801743
148.606765	2575.570260	5.882752	-0.029194	2.805800
148.772039	2583.631285	5.887757	-0.029230	2.809866
149.148097	2591.683585	5.892762	-0.029305	2.813934
149.483866	2599.708169	5.897766	-0.029373	2.817980
149.658167	2607.764851	5.902771	-0.029410	2.822027
149.820778	2615.819551	5.907776	-0.029446	2.826066
150.206877	2623.862232	5.912781	-0.029523	2.830106
150.513814	2631.928155	5.917786	-0.029585	2.834147
150.754618	2639.929258	5.922790	-0.029635	2.838147
151.042370	2647.952783	5.927795	-0.029694	2.842155
151.254557	2655.986305	5.932800	-0.029738	2.846157
151.621551	2664.023183	5.937805	-0.029812	2.850165
151.869760	2672.083114	5.942810	-0.029863	2.854171
152.289031	2680.109320	5.947814	-0.029946	2.858165
152.473227	2688.164609	5.952819	-0.029986	2.862154
152.601363	2696.188780	5.957824	-0.030015	2.866120
152.920957	2704.246415	5.962829	-0.030080	2.870106
153.073396	2712.310663	5.967834	-0.030113	2.874082
153.682285	2720.312224	5.972838	-0.030232	2.878046
153.838214	2728.355981	5.977843	-0.030266	2.882000
153.949816	2736.388395	5.982848	-0.030292	2.885941
154.370871	2744.436385	5.987853	-0.030375	2.889901
154.563087	2752.483333	5.992858	-0.030416	2.893842
154.979627	2760.533786	5.997862	-0.030499	2.897792
155.255148	2768.582206	6.002867	-0.030556	2.901728
155.622777	2776.572458	6.007872	-0.030629	2.905635
155.936881	2784.634228	6.012877	-0.030693	2.909569
156.275739	2792.734624	6.017882	-0.030761	2.913517
156.734302	2800.747293	6.022886	-0.030852	2.917424
156.939746	2808.779998	6.027891	-0.030895	2.921322
157.051745	2816.781413	6.032896	-0.030921	2.925195
157.477298	2824.809075	6.037901	-0.031005	2.929091
157.746988	2832.858184	6.042906	-0.031061	2.932985
157.958948	2840.930269	6.047910	-0.031105	2.936881
158.131955	2848.971283	6.052915	-0.031143	2.940755
158.500198	2856.947147	6.057920	-0.031216	2.944603
158.618118	2865.034398	6.062925	-0.031244	2.948486
158.866978	2873.065370	6.067930	-0.031295	2.952344
159.097262	2881.119444	6.072934	-0.031343	2.956207
159.349129	2889.133444	6.077939	-0.031395	2.960047
159.632832	2897.142121	6.082944	-0.031453	2.963880
159.951879	2905.202790	6.087949	-0.031518	2.967736
160.179566	2913.257634	6.092954	-0.031565	2.971579
160.473327	2921.308075	6.097958	-0.031625	2.975418
160.746032	2929.315352	6.102963	-0.031681	2.979230
160.940464	2937.346652	6.107968	-0.031722	2.983045
161.198423	2945.416576	6.112973	-0.031776	2.986877
161.263835	2953.457295	6.117978	-0.031793	2.990680
161.700813	2961.521863	6.122982	-0.031880	2.994508
161.943571	2969.522100	6.127987	-0.031930	2.998292
161.974540	2977.545648	6.132992	-0.031941	3.002071
162.306762	2985.580799	6.137997	-0.032008	3.005865
162.644707	2993.582441	6.143002	-0.032076	3.009639
162.894986	3001.634822	6.148006	-0.032128	3.013428
162.946734	3009.716949	6.153011	-0.032142	3.017216
163.275205	3017.712206	6.158016	-0.032209	3.020973
163.653296	3025.729795	6.163021	-0.032284	3.024737
163.781214	3033.786328	6.168026	-0.032313	3.028503
163.942724	3041.856170	6.173030	-0.032349	3.032272
164.241860	3049.905746	6.178035	-0.032409	3.036033
164.374646	3057.869820	6.183040	-0.032439	3.039742
164.655061	3065.919922	6.188045	-0.032497	3.043494
164.924518	3073.942170	6.193050	-0.032552	3.047227
165.129493	3082.003979	6.198054	-0.032595	3.050971
165.469282	3090.055184	6.203059	-0.032664	3.054712
165.643793	3098.063095	6.208064	-0.032701	3.058420
165.880890	3106.142777	6.213069	-0.032751	3.062160
166.140623	3114.147466	6.218074	-0.032804	3.065862
166.694388	3122.131277	6.223078	-0.032912	3.069563
167.065263	3130.267981	6.228083	-0.032987	3.073322
167.211992	3138.298187	6.233088	-0.033019	3.077016
167.476472	3146.305063	6.238093	-0.033074	3.080701
167.597530	3154.300738	6.243098	-0.033101	3.084370
167.916794	3162.321462	6.248102	-0.033166	3.088055
168.142333	3170.391469	6.253107	-0.033213	3.091753
168.550367	3178.398136	6.258112	-0.033294	3.095427
168.963064	3186.420228	6.263117	-0.033376	3.099103
169.213692	3194.440196	6.268122	-0.033428	3.102767
169.678659	3202.475790	6.273126	-0.033520	3.106443
169.901898	3210.525360	6.278131	-0.033566	3.110110
170.102863	3218.553729	6.283136	-0.033609	3.113762
170.452942	3226.618144	6.288141	-0.033679	3.117433
170.766539	3234.648951	6.293146	-0.033743	3.121083
170.797055	3242.648303	6.298150	-0.033754	3.124701
170.997746	3250.725185	6.303155	-0.033796	3.128358
171.218098	3258.753594	6.308160	-0.033842	3.131990
171.503192	3266.814177	6.313165	-0.033901	3.135634
171.568200	3274.839305	6.318170	-0.033918	3.139249
171.811301	3282.838866	6.323174	-0.033968	3.142856
172.133697	3290.897024	6.328179	-0.034033	3.146488
172.312986	3298.898558	6.333184	-0.034072	3.150085
172.663478	3306.994433	6.338189	-0.034142	3.153727
172.936608	3315.007555	6.343194	-0.034198	3.157324
173.208650	3323.020979	6.348198	-0.034254	3.160918
173.552950	3330.999572	6.353203	-0.034323	3.164495
173.678631	3339.047762	6.358208	-0.034352	3.168089
173.934489	3347.108014	6.363213	-0.034405	3.171690
173.903152	3355.151892	6.368218	-0.034404	3.175268
174.262884	3363.145415	6.373222	-0.034476	3.178836
174.651068	3371.191111	6.378227	-0.034554	3.182424
174.813772	3379.207815	6.383232	-0.034589	3.185985
175.078373	3387.251338	6.388237	-0.034644	3.189559
175.313908	3395.298322	6.393242	-0.034693	3.193129
175.508786	3403.329327	6.398246	-0.034734	3.196686
175.627369	3411.354694	6.403251	-0.034761	3.200234
175.908211	3419.368683	6.408256	-0.034819	3.203779
176.201580	3427.403983	6.413261	-0.034879	3.207330
176.445403	3435.444502	6.418266	-0.034929	3.210878
176.815894	3443.477835	6.423270	-0.035003	3.214424
177.235801	3451.487115	6.428275	-0.035087	3.217957
177.552952	3459.531443	6.433280	-0.035151	3.221497
177.918952	3467.523154	6.438285	-0.035224	3.225013
178.132856	3475.590109	6.443290	-0.035269	3.228551
178.432465	3483.668752	6.448294	-0.035330	3.232094
178.555739	3491.749933	6.453299	-0.035358	3.235626
178.841057	3499.708916	6.458304	-0.035416	3.239109
179.300186	3507.702087	6.463309	-0.035507	3.242609
179.564007	3515.702813	6.468314	-0.035561	3.246101
179.695809	3523.746037	6.473318	-0.035591	3.249602
180.042809	3531.810557	6.478323	-0.035661	3.253118
180.103693	3539.861304	6.483328	-0.035677	3.256612
180.251129	3547.861605	6.488333	-0.035710	3.260084
180.445675	3555.905176	6.493338	-0.035751	3.263573
180.633730	3563.909638	6.498342	-0.035791	3.267041
180.824607	3571.972355	6.503347	-0.035832	3.270530
180.864664	3580.019123	6.508352	-0.035845	3.274003
181.166406	3588.031141	6.513357	-0.035906	3.277467
181.502683	3596.030522	6.518362	-0.035974	3.280924
181.679931	3604.023825	6.523366	-0.036012	3.284368
182.061264	3612.058108	6.528371	-0.036088	3.287834
182.282811	3620.097240	6.533376	-0.036134	3.291293
182.421469	3628.176431	6.538381	-0.036165	3.294761
182.617469	3636.205092	6.543386	-0.036207	3.298207
182.958063	3644.224943	6.548390	-0.036276	3.301650
183.372723	3652.228457	6.553395	-0.036358	3.305086
183.540118	3660.274952	6.558400	-0.036394	3.308527
183.791481	3668.339304	6.563405	-0.036446	3.311975
183.969943	3676.356318	6.568410	-0.036485	3.315397
184.115683	3684.350833	6.573414	-0.036517	3.318804
184.424178	3692.376023	6.578419	-0.036580	3.322227
184.618497	3700.383652	6.583424	-0.036621	3.325635
184.872584	3708.403180	6.588429	-0.036673	3.329046
184.802862	3716.485977	6.593434	-0.036666	3.332469
185.215448	3724.524552	6.598438	-0.036748	3.335887
185.588095	3732.514496	6.603443	-0.036822	3.339280
185.920408	3740.542139	6.608448	-0.036889	3.342684
186.208600	3748.578262	6.613453	-0.036948	3.346086
186.483315	3756.580164	6.618458	-0.037004	3.349469
186.686892	3764.640944	6.623462	-0.037047	3.352872
187.163015	3772.708035	6.628467	-0.037141	3.356283
187.314317	3780.681473	6.633472	-0.037174	3.359640
187.637809	3788.703225	6.638477	-0.037240	3.363020
187.662402	3796.752117	6.643482	-0.037250	3.366397
188.080658	3804.761293	6.648486	-0.037333	3.369768
188.277557	3812.843838	6.653491	-0.037374	3.373158
188.478876	3820.838634	6.658496	-0.037417	3.376509
188.825876	3828.873216	6.663501	-0.037487	3.379878
189.260716	3836.863641	6.668506	-0.037573	3.383228
189.467427	3844.908449	6.673510	-0.037617	3.386590
189.803146	3852.947477	6.678515	-0.037684	3.389950
190.017902	3861.043858	6.683520	-0.037729	3.393326
190.477665	3869.088025	6.688525	-0.037820	3.396686
190.667467	3877.038879	6.693530	-0.037861	3.399995
191.065205	3885.030646	6.698534	-0.037940	3.403324
191.500696	3893.059693	6.703539	-0.038026	3.406667
191.712854	3901.052794	6.708544	-0.038071	3.409983
192.009069	3909.120813	6.713549	-0.038131	3.413331
192.248733	3917.185706	6.718554	-0.038181	3.416672
192.377215	3925.155812	6.723558	-0.038210	3.419966
192.851789	3933.193775	6.728563	-0.038303	3.423297
192.859949	3941.225813	6.733568	-0.038310	3.426607
193.313458	3949.252644	6.738573	-0.038400	3.429926
193.547631	3957.318321	6.743578	-0.038448	3.433251
193.625739	3965.343079	6.748582	-0.038468	3.436550
193.704405	3973.365654	6.753587	-0.038488	3.439846
193.971976	3981.312829	6.758592	-0.038543	3.443113
194.323571	3989.411855	6.763597	-0.038613	3.446442
194.612826	3997.398748	6.768602	-0.038672	3.449721
194.863820	4005.467515	6.773606	-0.038724	3.453028
195.060912	4013.520946	6.778611	-0.038766	3.456324
195.406570	4021.493701	6.783616	-0.038836	3.459588
195.515820	4029.554366	6.788621	-0.038861	3.462878
195.531916	4037.594145	6.793626	-0.038869	3.466153
195.947322	4045.602068	6.798630	-0.038952	3.469425
196.227520	4053.687656	6.803635	-0.039009	3.472721
196.329500	4061.695971	6.808640	-0.039033	3.475976
196.786733	4069.662211	6.813645	-0.039124	3.479223
196.967123	4077.697238	6.818650	-0.039162	3.482486
197.128987	4085.695844	6.823654	-0.039198	3.485730
197.247023	4093.750198	6.828659	-0.039225	3.488993
197.436184	4101.764085	6.833664	-0.039265	3.492238
197.588296	4109.839462	6.838669	-0.039299	3.495504
197.758814	4117.824263	6.843674	-0.039336	3.498731
197.951819	4125.848095	6.848678	-0.039377	3.501971
198.303441	4133.826831	6.853683	-0.039447	3.505195
198.439026	4141.874808	6.858688	-0.039478	3.508438
198.805841	4149.940444	6.863693	-0.039551	3.511691
199.192609	4157.963981	6.868698	-0.039628	3.514925
199.356722	4165.941329	6.873702	-0.039664	3.518131
199.403037	4174.007514	6.878707	-0.039678	3.521366
199.611334	4181.969731	6.883712	-0.039722	3.524561
199.893579	4190.021078	6.888717	-0.039779	3.527791
199.941236	4198.059465	6.893722	-0.039793	3.531005
200.210243	4206.116598	6.898726	-0.039849	3.534231
200.638858	4214.167601	6.903731	-0.039934	3.537457
200.701271	4222.151890	6.908736	-0.039950	3.540641
200.892894	4230.173688	6.913741	-0.039991	3.543842
201.290105	4238.218820	6.918746	-0.040070	3.547055
201.390446	4246.231564	6.923750	-0.040094	3.550244
201.686693	4254.380074	6.928755	-0.040155	3.553489
201.943646	4262.370663	6.933760	-0.040207	3.556668
202.241802	4270.307171	6.938765	-0.040268	3.559823
202.316202	4278.362035	6.943770	-0.040287	3.563016
202.631221	4286.349588	6.948774	-0.040351	3.566186
202.861678	4294.372740	6.953779	-0.040399	3.569365
202.967880	4302.409904	6.958784	-0.040424	3.572544
203.120510	4310.438221	6.963789	-0.040457	3.575717
203.380270	4318.435035	6.968794	-0.040511	3.578878
203.478141	4326.487297	6.973798	-0.040534	3.582053
203.601036	4334.500505	6.978803	-0.040562	3.585211
203.603080	4342.520858	6.983808	-0.040568	3.588366
203.986926	4350.581902	6.988813	-0.040645	3.591544
204.260658	4358.580236	6.993818	-0.040701	3.594692
204.297234	4366.592398	6.998822	-0.040713	3.597836
204.674465	4374.608702	7.003827	-0.040788	3.600988
204.720239	4382.593674	7.008832	-0.040802	3.604116
204.886770	4390.651251	7.013837	-0.040838	3.607273
205.268385	4398.657538	7.018842	-0.040914	3.610413
205.549414	4406.700494	7.023846	-0.040971	3.613562
205.854023	4414.772948	7.028851	-0.041033	3.616720
205.939892	4422.728615	7.033856	-0.041054	3.619824
206.338210	4430.775845	7.038861	-0.041134	3.622970
206.419011	4438.801945	7.043866	-0.041154	3.626095
206.575650	4446.826501	7.048870	-0.041188	3.629220
207.078523	4454.874117	7.053875	-0.041287	3.632360
206.820615	4462.950421	7.058880	-0.041244	3.635488
207.288632	4470.922863	7.063885	-0.041337	3.638592
207.578849	4478.960562	7.068890	-0.041396	3.641715
207.950144	4486.898867	7.073894	-0.041470	3.644798
207.914080	4494.994787	7.078899	-0.041468	3.647929
207.913472	4503.016837	7.083904	-0.041473	3.651029
208.297155	4511.064747	7.088909	-0.041550	3.654147
208.678190	4519.060797	7.093914	-0.041626	3.657242
208.740457	4527.064389	7.098918	-0.041643	3.660329
209.057990	4535.115863	7.103923	-0.041707	3.663439
209.287111	4543.138909	7.108928	-0.041755	3.666532
209.339122	4551.127159	7.113933	-0.041770	3.669605
209.700047	4559.198943	7.118938	-0.041842	3.672716
209.692401	4567.233260	7.123942	-0.041846	3.675800
209.980064	4575.214707	7.128947	-0.041905	3.678868
210.051505	4583.239353	7.133952	-0.041923	3.681945
210.317771	4591.222744	7.138957	-0.041978	3.685009
210.457809	4599.285751	7.143962	-0.042009	3.688097
210.480443	4607.284079	7.148966	-0.042018	3.691155
210.754913	4615.363256	7.153971	-0.042075	3.694248
211.020290	4623.345988	7.158976	-0.042129	3.697301
211.312545	4631.351705	7.163981	-0.042189	3.700361
211.622547	4639.380243	7.168986	-0.042252	3.703427
211.703019	4647.429683	7.173990	-0.042272	3.706493
211.941413	4655.434535	7.178995	-0.042321	3.709544
211.870910	4663.534265	7.184000	-0.042313	3.712620
212.365646	4671.556565	7.189005	-0.042411	3.715679
212.861805	4679.509049	7.194010	-0.042508	3.718708
212.911042	4687.526525	7.199014	-0.042522	3.721748
213.373131	4695.493718	7.204019	-0.042614	3.724777
213.524526	4703.508013	7.209024	-0.042647	3.727814
213.808998	4711.566724	7.214029	-0.042705	3.730868
214.050644	4719.626616	7.219034	-0.042755	3.733920
214.203221	4727.640093	7.224038	-0.042789	3.736949
214.399913	4735.650749	7.229043	-0.042831	3.739975
214.585049	4743.669540	7.234048	-0.042870	3.743002
214.616689	4751.692061	7.239053	-0.042881	3.746024
214.887867	4759.690391	7.244058	-0.042937	3.749040
214.963589	4767.775539	7.249062	-0.042956	3.752082
215.603764	4775.790785	7.254067	-0.043080	3.755108
215.663592	4783.776207	7.259072	-0.043097	3.758107
215.705008	4791.849943	7.264077	-0.043110	3.761136
215.952309	4799.817588	7.269082	-0.043161	3.764128
216.468275	4807.844492	7.274086	-0.043262	3.767146
216.793546	4815.889683	7.279091	-0.043328	3.770164
216.845251	4823.928008	7.284096	-0.043342	3.773170
217.137866	4831.984109	7.289101	-0.043402	3.776186
217.268389	4839.966201	7.294106	-0.043432	3.779169
217.264113	4847.984541	7.299110	-0.043436	3.782159
217.555133	4856.009968	7.304115	-0.043495	3.785157
217.857592	4864.004303	7.309120	-0.043557	3.788140
218.010376	4872.063518	7.314125	-0.043590	3.791142
218.426276	4880.106016	7.319130	-0.043673	3.794142
218.650042	4888.131965	7.324134	-0.043720	3.797128
218.920300	4896.116160	7.329139	-0.043775	3.800098
219.051903	4904.119085	7.334144	-0.043805	3.803069
219.363605	4912.126209	7.339149	-0.043868	3.806043
219.587886	4920.154964	7.344154	-0.043915	3.809022
219.707318	4928.199585	7.349158	-0.043942	3.812001
220.021965	4936.240926	7.354163	-0.044006	3.814981
220.215514	4944.255120	7.359168	-0.044047	3.817946
220.377917	4952.223283	7.364173	-0.044083	3.820891
220.530628	4960.258342	7.369178	-0.044116	3.823858
220.726483	4968.302330	7.374182	-0.044158	3.826827
220.962220	4976.313919	7.379187	-0.044207	3.829783
221.011949	4984.378021	7.384192	-0.044221	3.832751
221.187984	4992.380948	7.389197	-0.044259	3.835698
221.535375	5000.371091	7.394202	-0.044329	3.838641
221.669626	5008.403329	7.399206	-0.044359	3.841593
222.038703	5016.357991	7.404211	-0.044433	3.844519
222.177031	5024.422926	7.409216	-0.044464	3.847478
222.572094	5032.408228	7.414221	-0.044543	3.850411
222.850079	5040.497591	7.419226	-0.044600	3.853378
222.877511	5048.539701	7.424230	-0.044610	3.856320
223.180628	5056.514676	7.429235	-0.044671	3.859240
223.131371	5064.581021	7.434240	-0.044667	3.862185
223.279253	5072.551146	7.439245	-0.044700	3.865096
223.744430	5080.601714	7.444250	-0.044792	3.868041
223.836514	5088.623161	7.449254	-0.044814	3.870965
224.313333	5096.880409	7.454259	-0.044908	3.873981
224.403447	5104.865516	7.459264	-0.044930	3.876887
224.727589	5112.761612	7.464269	-0.044996	3.879764
224.893510	5120.742684	7.469274	-0.045032	3.882666
225.134854	5128.724063	7.474278	-0.045082	3.885568
225.495079	5136.782706	7.479283	-0.045154	3.888497
225.589547	5144.781507	7.484288	-0.045177	3.891398
225.749819	5152.834600	7.489293	-0.045212	3.894317
226.133719	5160.835457	7.494298	-0.045288	3.897220
226.178197	5168.812711	7.499302	-0.045302	3.900105
226.511629	5176.846522	7.504307	-0.045369	3.903014
226.570674	5184.868726	7.509312	-0.045385	3.905912
226.544500	5192.897001	7.514317	-0.045385	3.908808
226.927281	5200.925733	7.519322	-0.045462	3.911710
227.005466	5208.951102	7.524326	-0.045481	3.914602
227.410272	5216.974410	7.529331	-0.045562	3.917498
227.499872	5224.949574	7.534336	-0.045584	3.920368
227.547374	5232.976209	7.539341	-0.045598	3.923254
227.932299	5240.998670	7.544346	-0.045675	3.926143
227.916327	5249.001292	7.549350	-0.045677	3.929014
228.325603	5257.050252	7.554355	-0.045758	3.931909
228.722004	5265.042351	7.559360	-0.045837	3.934780
229.003705	5273.088037	7.564365	-0.045895	3.937666
229.111640	5281.086409	7.569370	-0.045920	3.940530
229.042342	5289.100285	7.574374	-0.045912	3.943395
229.427021	5297.110730	7.579379	-0.045989	3.946264
229.661229	5305.147672	7.584384	-0.046038	3.949138
229.914652	5313.203643	7.589389	-0.046090	3.952016
230.017199	5321.237026	7.594394	-0.046114	3.954882
230.336029	5329.236006	7.599398	-0.046179	3.957738
230.605474	5337.235393	7.604403	-0.046234	3.960590
230.787293	5345.232588	7.609408	-0.046273	3.963439
231.107736	5353.242163	7.614413	-0.046338	3.966292
231.141408	5361.305603	7.619418	-0.046349	3.969157
231.374000	5369.310022	7.624422	-0.046398	3.972002
231.602309	5377.370672	7.629427	-0.046445	3.974865
231.826692	5385.377512	7.634432	-0.046492	3.977707
232.067873	5393.383220	7.639437	-0.046542	3.980547
232.149047	5401.400460	7.644442	-0.046563	3.983386
232.168971	5409.394522	7.649446	-0.046571	3.986214
232.494643	5417.474664	7.654451	-0.046637	3.989075
232.571169	5425.487354	7.659456	-0.046657	3.991907
232.888031	5433.524824	7.664461	-0.046721	3.994749
233.038234	5441.595258	7.669466	-0.046754	3.997597
233.130329	5449.553651	7.674470	-0.046776	4.000404
233.583021	5457.563408	7.679475	-0.046866	4.003232
233.763173	5465.535420	7.684480	-0.046904	4.006041
233.885443	5473.569879	7.689485	-0.046932	4.008868
234.006491	5481.654556	7.694490	-0.046960	4.011711
234.168340	5489.668511	7.699494	-0.046995	4.014528
234.326983	5497.707889	7.704499	-0.047030	4.017352
234.296392	5505.666066	7.709504	-0.047029	4.020143
234.687096	5513.669171	7.714509	-0.047107	4.022953
234.794866	5521.692211	7.719514	-0.047132	4.025765
235.131834	5529.703785	7.724518	-0.047200	4.028574
235.501011	5537.779538	7.729523	-0.047274	4.031403
235.751511	5545.876977	7.734528	-0.047326	4.034237
235.744031	5553.893829	7.739533	-0.047330	4.037036
236.052812	5561.799801	7.744538	-0.047392	4.039800
236.193954	5569.816972	7.749542	-0.047424	4.042598
236.419129	5577.829928	7.754547	-0.047471	4.045394
236.517243	5585.842232	7.759552	-0.047494	4.048185
236.853120	5593.851025	7.764557	-0.047562	4.050977
236.977457	5601.938996	7.769562	-0.047590	4.053792
237.001624	5609.933467	7.774566	-0.047600	4.056570
237.479467	5617.928134	7.779571	-0.047694	4.059354
237.705834	5625.907365	7.784576	-0.047741	4.062126
237.858596	5633.920383	7.789581	-0.047775	4.064907
237.871648	5641.991527	7.794586	-0.047783	4.067704
238.130975	5650.014943	7.799590	-0.047836	4.070487
238.305052	5658.060949	7.804595	-0.047874	4.073274
238.478837	5666.055667	7.809600	-0.047911	4.076041
238.590135	5674.043942	7.814605	-0.047937	4.078804
238.788048	5682.061361	7.819610	-0.047979	4.081575
238.834277	5690.032424	7.824614	-0.047993	4.084327
239.056957	5698.136842	7.829619	-0.048039	4.087125
239.252536	5706.094844	7.834624	-0.048081	4.089871
239.720438	5714.152819	7.839629	-0.048173	4.092652
239.701689	5722.208185	7.844634	-0.048175	4.095425
240.109628	5730.167147	7.849638	-0.048256	4.098168
240.606654	5738.182704	7.854643	-0.048354	4.100929
240.519783	5746.209878	7.859648	-0.048342	4.103686
240.689633	5754.250833	7.864653	-0.048379	4.106448
241.010373	5762.280633	7.869658	-0.048444	4.109207
240.962975	5770.309813	7.874662	-0.048440	4.111958
241.210475	5778.351526	7.879667	-0.048492	4.114716
241.361332	5786.385018	7.884672	-0.048525	4.117468
241.574840	5794.340381	7.889677	-0.048570	4.120193
241.646673	5802.383985	7.894682	-0.048588	4.122943
241.774579	5810.357808	7.899686	-0.048617	4.125669
242.023640	5818.417606	7.904691	-0.048669	4.128424
242.184211	5826.444925	7.909696	-0.048704	4.131165
242.463814	5834.468764	7.914701	-0.048761	4.133904
242.868146	5842.530225	7.919706	-0.048842	4.136656
242.851863	5850.449932	7.924710	-0.048844	4.139352
242.949223	5858.543305	7.929715	-0.048867	4.142107
243.086608	5866.525897	7.934720	-0.048898	4.144824
243.374012	5874.566408	7.939725	-0.048956	4.147559
243.557235	5882.604045	7.944730	-0.048996	4.150291
243.738811	5890.640675	7.949734	-0.049035	4.153021
243.988447	5898.678479	7.954739	-0.049086	4.155750
244.079018	5906.630397	7.959744	-0.049108	4.158446
244.234231	5914.661838	7.964749	-0.049142	4.161168
244.497371	5922.673716	7.969754	-0.049196	4.163883
244.532787	5930.680177	7.974758	-0.049208	4.166591
244.994905	5938.744038	7.979763	-0.049299	4.169323
245.150452	5946.709923	7.984768	-0.049333	4.172015
245.393991	5954.767834	7.989773	-0.049384	4.174738
245.565338	5962.792768	7.994778	-0.049421	4.177448
245.827010	5970.744992	7.999782	-0.049475	4.180132
246.136067	5978.766704	8.004787	-0.049537	4.182838
246.304135	5986.755656	8.009792	-0.049574	4.185529
246.494699	5994.799219	8.014797	-0.049615	4.188238
246.749537	6002.862730	8.019802	-0.049667	4.190952
246.832099	6010.977034	8.024806	-0.049688	4.193680
246.992832	6018.973294	8.029811	-0.049723	4.196367
247.046645	6026.948341	8.034816	-0.049738	4.199044
247.324968	6034.903791	8.039821	-0.049795	4.201716
247.593749	6042.928078	8.044826	-0.049850	4.204408
247.505697	6050.925766	8.049830	-0.049839	4.207086
247.987414	6058.898896	8.054835	-0.049934	4.209760
248.010682	6066.970638	8.059840	-0.049943	4.212461
248.182050	6074.974895	8.064845	-0.049980	4.215138
248.531465	6082.992977	8.069850	-0.050050	4.217821
248.538600	6091.003174	8.074854	-0.050057	4.220495
248.637713	6099.029766	8.079859	-0.050080	4.223175
248.803617	6107.090435	8.084864	-0.050116	4.225864
249.010024	6115.016433	8.089869	-0.050160	4.228508
249.191825	6123.093544	8.094874	-0.050199	4.231199
249.346140	6131.119439	8.099878	-0.050233	4.233872
249.881291	6139.200554	8.104883	-0.050338	4.236565
250.050623	6147.134949	8.109888	-0.050374	4.239204
250.142922	6155.184660	8.114893	-0.050397	4.241879
250.343290	6163.166842	8.119898	-0.050439	4.244531
250.596912	6171.180853	8.124902	-0.050492	4.247192
250.538428	6179.219032	8.129907	-0.050486	4.249857
250.829910	6187.254470	8.134912	-0.050545	4.252522
251.104213	6195.272912	8.139917	-0.050601	4.255180
251.232032	6203.324062	8.144922	-0.050630	4.257845
251.415038	6211.289120	8.149926	-0.050670	4.260481
251.504495	6219.372249	8.154931	-0.050691	4.263154
251.665439	6227.293137	8.159936	-0.050726	4.265772
251.739149	6235.331953	8.164941	-0.050745	4.268426
251.980603	6243.424424	8.169946	-0.050796	4.271098
252.090651	6251.455393	8.174950	-0.050821	4.273746
252.290148	6259.491928	8.179955	-0.050863	4.276396
252.412175	6267.431197	8.184960	-0.050891	4.279011
252.605429	6275.439997	8.189965	-0.050932	4.281648
252.970019	6283.456140	8.194970	-0.051005	4.284288
252.949894	6291.455665	8.199974	-0.051007	4.286917
253.289892	6299.492030	8.204979	-0.051075	4.289559
253.391238	6307.539382	8.209984	-0.051099	4.292202
253.395999	6315.554123	8.214989	-0.051105	4.294831
253.620068	6323.628471	8.219994	-0.051152	4.297480
253.777770	6331.555091	8.224998	-0.051187	4.300079
254.125985	6339.624128	8.230003	-0.051257	4.302724
254.083198	6347.578710	8.235008	-0.051254	4.305326
254.407464	6355.596313	8.240013	-0.051319	4.307951
254.447321	6363.659013	8.245018	-0.051332	4.310587
254.658941	6371.674899	8.250022	-0.051377	4.313207
254.926666	6379.716470	8.255027	-0.051432	4.315834
254.977242	6387.718212	8.260032	-0.051446	4.318445
255.154094	6395.675048	8.265037	-0.051484	4.321040
255.407665	6403.726081	8.270042	-0.051537	4.323666
255.798978	6411.727284	8.275046	-0.051615	4.326274
255.860797	6419.750304	8.280051	-0.051631	4.328886
255.938823	6427.783610	8.285056	-0.051651	4.331499
256.257063	6435.801259	8.290061	-0.051715	4.334107
256.383176	6443.868351	8.295066	-0.051744	4.336729
256.490830	6451.834963	8.300070	-0.051769	4.339316
256.830959	6459.864069	8.305075	-0.051838	4.341924
256.857679	6467.840129	8.310080	-0.051848	4.344510
256.939185	6475.867051	8.315085	-0.051868	4.347112
257.206296	6483.896968	8.320090	-0.051923	4.349715
257.488735	6491.918958	8.325094	-0.051981	4.352313
257.493697	6500.041190	8.330099	-0.051987	4.354941
257.535995	6508.035260	8.335104	-0.052000	4.357525
257.717195	6515.947288	8.340109	-0.052039	4.360083
258.014527	6523.943025	8.345114	-0.052099	4.362667
257.895816	6531.912914	8.350118	-0.052082	4.365238
258.294488	6539.989942	8.355123	-0.052161	4.367845
258.565425	6548.004611	8.360128	-0.052217	4.370430
258.712727	6556.042924	8.365133	-0.052250	4.373021
258.940066	6564.073925	8.370138	-0.052297	4.375608
259.122868	6572.022264	8.375142	-0.052336	4.378166
259.139485	6580.092929	8.380147	-0.052345	4.380761
259.369142	6588.105316	8.385152	-0.052392	4.383338
259.671459	6596.129011	8.390157	-0.052454	4.385916
259.862918	6604.148791	8.395162	-0.052495	4.388492
259.775565	6612.126584	8.400166	-0.052484	4.391051
259.990838	6620.213905	8.405171	-0.052529	4.393645
260.257447	6628.252604	8.410176	-0.052584	4.396222
260.289707	6636.187894	8.415181	-0.052595	4.398763
260.249527	6644.273400	8.420186	-0.052592	4.401351
260.588986	6652.216879	8.425190	-0.052661	4.403893
261.068245	6660.240995	8.430195	-0.052755	4.406461
261.161426	6668.278081	8.435200	-0.052778	4.409029
261.271142	6676.284428	8.440205	-0.052803	4.411586
261.337245	6684.333336	8.445210	-0.052821	4.414155
261.425401	6692.354315	8.450214	-0.052842	4.416713
261.755075	6700.376336	8.455219	-0.052909	4.419272
261.997882	6708.411303	8.460224	-0.052959	4.421832
261.950082	6716.398418	8.465229	-0.052955	4.424375
261.993153	6724.463389	8.470234	-0.052969	4.426941
262.155591	6732.406630	8.475238	-0.053004	4.429468
262.382070	6740.473454	8.480243	-0.053051	4.432033
262.662493	6748.495136	8.485248	-0.053109	4.434582
262.948793	6756.544098	8.490253	-0.053167	4.437138
262.996625	6764.483919	8.495258	-0.053181	4.439657
263.187011	6772.548499	8.500262	-0.053222	4.442215
263.286352	6780.517505	8.505267	-0.053245	4.444741
263.672410	6788.583018	8.510272	-0.053322	4.447297
263.836476	6796.524946	8.515277	-0.053358	4.449811
263.996840	6804.611668	8.520282	-0.053393	4.452370
263.904996	6812.607460	8.525286	-0.053381	4.454897
264.370759	6820.655323	8.530291	-0.053473	4.457442
264.431303	6828.615928	8.535296	-0.053489	4.459956
264.472008	6836.615920	8.540301	-0.053502	4.462481
264.733796	6844.639682	8.545306	-0.053556	4.465013
265.022674	6852.670771	8.550310	-0.053615	4.467546
265.096721	6860.703004	8.555315	-0.053634	4.470077
265.264805	6868.754656	8.560320	-0.053670	4.472613
265.301243	6876.768718	8.565325	-0.053682	4.475136
265.440022	6884.787227	8.570330	-0.053713	4.477658
265.743022	6892.743040	8.575335	-0.053775	4.480160
265.990263	6900.776559	8.580339	-0.053826	4.482685
266.058545	6908.756839	8.585344	-0.053844	4.485191
266.207299	6916.784607	8.590349	-0.053877	4.487711
266.669821	6924.807948	8.595354	-0.053968	4.490229
266.732917	6932.817847	8.600359	-0.053985	4.492740
266.774305	6940.907220	8.605363	-0.053998	4.495274
266.845360	6948.881230	8.610368	-0.054016	4.497771
267.215324	6956.888985	8.615373	-0.054090	4.500278
267.141730	6964.895227	8.620378	-0.054081	4.502782
267.323098	6972.841798	8.625383	-0.054120	4.505266
267.781513	6980.945473	8.630387	-0.054211	4.507799
267.732464	6988.974992	8.635392	-0.054207	4.510306
267.672993	6997.018056	8.640397	-0.054201	4.512816
268.130478	7005.110659	8.645402	-0.054291	4.515341
268.156227	7013.004843	8.650407	-0.054301	4.517802
268.540531	7021.009984	8.655411	-0.054378	4.520297
268.614430	7029.024928	8.660416	-0.054397	4.522792
268.695057	7036.981067	8.665421	-0.054417	4.525268
269.039632	7045.042239	8.670426	-0.054486	4.527776
269.124586	7053.027343	8.675431	-0.054507	4.530259
269.316066	7061.093590	8.680435	-0.054548	4.532765
269.550155	7069.104783	8.685440	-0.054597	4.535253
269.678424	7077.117081	8.690445	-0.054626	4.537739
270.030730	7085.132540	8.695450	-0.054697	4.540226
270.064892	7093.138191	8.700455	-0.054708	4.542708
270.251808	7101.131293	8.705459	-0.054748	4.545185
270.560070	7109.155437	8.710464	-0.054811	4.547670
270.669304	7117.187110	8.715469	-0.054836	4.550155
270.713183	7125.223537	8.720474	-0.054849	4.552641
270.768812	7133.225940	8.725479	-0.054865	4.555115
270.998316	7141.274409	8.730483	-0.054913	4.557602
271.246335	7149.235265	8.735488	-0.054964	4.560061
271.299092	7157.265052	8.740493	-0.054979	4.562539
271.633460	7165.255637	8.745498	-0.055046	4.565004
271.864632	7173.306766	8.750503	-0.055095	4.567486
271.808529	7181.315722	8.755507	-0.055089	4.569954
271.845681	7189.365197	8.760512	-0.055101	4.572433
272.099134	7197.367675	8.765517	-0.055154	4.574896
272.365531	7205.444584	8.770522	-0.055208	4.577381
272.374246	7213.332669	8.775527	-0.055215	4.579806
272.792574	7221.474964	8.780531	-0.055298	4.582308
272.867736	7229.390814	8.785536	-0.055317	4.584739
272.847867	7237.466759	8.790541	-0.055319	4.587218
273.074297	7245.465177	8.795546	-0.055366	4.589672
273.169899	7253.506892	8.800551	-0.055389	4.592138
273.491777	7261.555699	8.805555	-0.055454	4.594605
273.449912	7269.591077	8.810560	-0.055452	4.597066
273.951407	7277.504685	8.815565	-0.055550	4.599488
273.883302	7285.589547	8.820570	-0.055543	4.601962
274.025895	7293.476388	8.825575	-0.055574	4.604374
274.341324	7301.578849	8.830579	-0.055638	4.606850
274.452289	7309.594875	8.835584	-0.055664	4.609299
274.498635	7317.615221	8.840589	-0.055678	4.611747
274.842421	7325.669560	8.845594	-0.055747	4.614205
274.974479	7333.669909	8.850599	-0.055777	4.616645
275.159298	7341.618225	8.855603	-0.055816	4.619067
274.995288	7349.671017	8.860608	-0.055791	4.621521
275.164724	7357.613450	8.865613	-0.055827	4.623939
275.652026	7365.712322	8.870618	-0.055923	4.626403
275.888381	7373.704511	8.875623	-0.055972	4.628834
276.106930	7381.784183	8.880627	-0.056018	4.631290
276.208668	7389.786848	8.885632	-0.056042	4.633722
276.213363	7397.783301	8.890637	-0.056048	4.636150
276.446197	7405.771044	8.895642	-0.056097	4.638574
276.545088	7413.771000	8.900647	-0.056120	4.641001
276.684376	7421.816487	8.905651	-0.056152	4.643440
276.760199	7429.805299	8.910656	-0.056171	4.645861
277.078671	7437.839208	8.915661	-0.056235	4.648294
277.263211	7445.845075	8.920666	-0.056275	4.650717
277.329547	7453.872365	8.925671	-0.056292	4.653146
277.607623	7461.898406	8.930675	-0.056349	4.655573
277.912945	7469.931947	8.935680	-0.056411	4.658000
278.023990	7477.910143	8.940685	-0.056437	4.660410
278.143924	7485.923585	8.945690	-0.056464	4.662829
278.333902	7493.857710	8.950695	-0.056505	4.665223
278.512272	7502.001988	8.955699	-0.056543	4.667679
278.464915	7510.034610	8.960704	-0.056540	4.670101
278.717848	7518.051054	8.965709	-0.056592	4.672516
278.971069	7526.149530	8.970714	-0.056644	4.674954
278.998423	7534.064411	8.975719	-0.056654	4.677336
279.079734	7542.019967	8.980723	-0.056675	4.679729
279.377592	7550.045230	8.985728	-0.056735	4.682141
279.239625	7557.977688	8.990733	-0.056715	4.684525
279.506286	7566.091215	8.995738	-0.056770	4.686962
279.652049	7574.023166	9.000743	-0.056802	4.689343
279.862986	7582.129274	9.005747	-0.056846	4.691774
280.052116	7590.126029	9.010752	-0.056887	4.694172
280.260139	7598.091654	9.015757	-0.056930	4.696559
280.623741	7606.158398	9.020762	-0.057003	4.698975
280.477347	7614.170543	9.025767	-0.056981	4.701374
280.588771	7622.160438	9.030771	-0.057007	4.703765
280.917868	7630.212457	9.035776	-0.057074	4.706173
280.916083	7638.188893	9.040781	-0.057078	4.708557
281.155823	7646.224583	9.045786	-0.057128	4.710958
281.262964	7654.240397	9.050791	-0.057153	4.713352
281.398420	7662.287769	9.055795	-0.057184	4.715753
281.514457	7670.292037	9.060800	-0.057210	4.718141
281.645198	7678.249224	9.065805	-0.057240	4.720513
281.955778	7686.314747	9.070810	-0.057303	4.722916
281.909714	7694.277494	9.075815	-0.057299	4.725289
282.231840	7702.345178	9.080819	-0.057364	4.727690
282.396597	7710.389377	9.085824	-0.057400	4.730083
282.521968	7718.376444	9.090829	-0.057429	4.732458
282.723740	7726.451319	9.095834	-0.057472	4.734858
282.936683	7734.448509	9.100839	-0.057516	4.737234
283.301899	7742.428225	9.105843	-0.057589	4.739602
283.330042	7750.476955	9.110848	-0.057600	4.741991
283.344569	7758.373833	9.115853	-0.057608	4.744334
283.580063	7766.537137	9.120858	-0.057657	4.746754
283.679882	7774.489318	9.125863	-0.057680	4.749110
283.915849	7782.517649	9.130867	-0.057729	4.751488
284.111328	7790.579171	9.135872	-0.057771	4.753874
284.372844	7798.515793	9.140877	-0.057825	4.756222
284.489377	7806.580377	9.145882	-0.057852	4.758607
284.373966	7814.520579	9.150887	-0.057835	4.760954
284.606548	7822.542877	9.155891	-0.057884	4.763324
284.847594	7830.594748	9.160896	-0.057934	4.765701
284.994982	7838.586089	9.165901	-0.057966	4.768059
285.265392	7846.631707	9.170906	-0.058022	4.770432
285.387363	7854.624454	9.175911	-0.058050	4.772789
285.674005	7862.673167	9.180915	-0.058108	4.775160
285.732322	7870.648750	9.185920	-0.058124	4.777509
285.840701	7878.670328	9.190925	-0.058150	4.779870
286.052787	7886.724934	9.195930	-0.058194	4.782240
286.211848	7894.622581	9.200935	-0.058229	4.784563
286.279135	7902.722521	9.205939	-0.058247	4.786944
286.603024	7910.728182	9.210944	-0.058312	4.789295
286.575452	7918.759392	9.215949	-0.058312	4.791654
286.736102	7926.779239	9.220954	-0.058347	4.794008
286.826545	7934.782895	9.225959	-0.058369	4.796356
287.096527	7942.755957	9.230963	-0.058425	4.798693
287.335745	7950.820967	9.235968	-0.058474	4.801056
287.480590	7958.783070	9.240973	-0.058506	4.803388
287.599402	7966.847870	9.245978	-0.058534	4.805749
287.787317	7974.824966	9.250983	-0.058574	4.808083
288.169034	7982.865704	9.255987	-0.058650	4.810434
288.193477	7990.384636	9.260992	-0.058659	4.812632
288.346340	7994.858037	9.265997	-0.058691	4.813939
288.469363	7997.183573	9.271002	-0.058715	4.814618
288.671754	7998.539501	9.276007	-0.058753	4.815013
288.881070	7999.226769	9.281011	-0.058793	4.815213
288.877043	7999.752410	9.286016	-0.058792	4.815367
288.818005	7999.737539	9.291021	-0.058781	4.815363
289.002159	7999.776897	9.296026	-0.058815	4.815373
289.000637	7999.751220	9.301031	-0.058815	4.815366
289.057715	7999.750016	9.306035	-0.058826	4.815365
289.111229	7999.808593	9.311040	-0.058836	4.815382
289.249569	7999.733930	9.316045	-0.058861	4.815360
289.203532	7999.799414	9.321050	-0.058853	4.815379
289.264781	7999.743784	9.326055	-0.058864	4.815362
289.498212	7999.746556	9.331059	-0.058907	4.815362
289.625680	7999.798872	9.336064	-0.058931	4.815377
289.611101	7999.716346	9.341069	-0.058928	4.815353
289.591609	7999.757691	9.346074	-0.058924	4.815365
289.556945	7999.769935	9.351079	-0.058918	4.815369
289.651169	7999.769344	9.356083	-0.058935	4.815368
289.873657	7999.814679	9.361088	-0.058977	4.815380
289.859516	7999.734296	9.366093	-0.058974	4.815357
289.928202	7999.732216	9.371098	-0.058987	4.815356
290.066332	7999.709909	9.376103	-0.059012	4.815349
290.300638	7999.769331	9.381107	-0.059056	4.815365
290.307818	7999.847449	9.386112	-0.059057	4.815388
290.126246	7999.736521	9.391117	-0.059023	4.815356
290.238071	7999.849490	9.396122	-0.059044	4.815389
290.171001	7999.808839	9.401127	-0.059031	4.815377
290.234792	7999.783170	9.406131	-0.059043	4.815369
290.334656	7999.773055	9.411136	-0.059062	4.815366
290.239451	7999.769341	9.416141	-0.059044	4.815365
290.424160	7999.852523	9.421146	-0.059078	4.815389
290.401325	7999.883129	9.426151	-0.059074	4.815398
290.265612	7999.753722	9.431155	-0.059049	4.815360
290.546957	7999.802167	9.436160	-0.059101	4.815373
290.615901	7999.801159	9.441165	-0.059114	4.815373
290.560474	7999.854736	9.446170	-0.059103	4.815389
290.325629	7999.829484	9.451175	-0.059059	4.815382
290.482569	7999.882289	9.456179	-0.059089	4.815397
290.573795	7999.884855	9.461184	-0.059106	4.815397
290.561425	7999.800225	9.466189	-0.059103	4.815373
290.632001	7999.849469	9.471194	-0.059116	4.815387
290.728280	7999.905548	9.476199	-0.059134	4.815403
290.849011	7999.854103	9.481203	-0.059156	4.815387
290.795845	7999.905580	9.486208	-0.059146	4.815402
290.870492	7999.802081	9.491213	-0.059160	4.815372
290.955746	7999.856910	9.496218	-0.059176	4.815387
290.870859	7999.884355	9.501223	-0.059160	4.815396
290.767847	7999.813190	9.506227	-0.059141	4.815375
290.973019	7999.895644	9.511232	-0.059179	4.815399
291.022660	7999.818448	9.516237	-0.059188	4.815376
291.206852	7999.892007	9.521242	-0.059222	4.815396
291.144067	7999.877072	9.526247	-0.059211	4.815392
290.997419	7999.847931	9.531251	-0.059183	4.815385
290.913958	7999.879673	9.536256	-0.059168	4.815394
290.847068	7999.877494	9.541261	-0.059155	4.815394
291.123420	7999.967535	9.546266	-0.059207	4.815419
291.060486	7999.838256	9.551271	-0.059195	4.815381
291.108102	7999.867887	9.556275	-0.059203	4.815390
291.035977	7999.879513	9.561280	-0.059190	4.815394
291.194473	7999.846857	9.566285	-0.059219	4.815383
291.194741	7999.901353	9.571290	-0.059219	4.815399
291.087526	7999.900646	9.576295	-0.059199	4.815399
291.095432	7999.838790	9.581299	-0.059201	4.815381
291.158983	7999.836626	9.586304	-0.059212	4.815380
291.140943	7999.859830	9.591309	-0.059209	4.815387
291.424189	7999.874114	9.596314	-0.059262	4.815390
291.305680	7999.866808	9.601319	-0.059240	4.815389
291.264931	7999.873609	9.606323	-0.059232	4.815391
291.457232	7999.943029	9.611328	-0.059268	4.815410
291.214472	7999.873831	9.616333	-0.059222	4.815391
291.328089	7999.946227	9.621338	-0.059243	4.815412
291.451470	7999.893756	9.626343	-0.059266	4.815396
291.341363	7999.843845	9.631347	-0.059246	4.815382
291.364358	7999.879481	9.636352	-0.059250	4.815392
291.515998	7999.822134	9.641357	-0.059278	4.815375
291.706541	7999.862672	9.646362	-0.059313	4.815385
291.378817	7999.861532	9.651367	-0.059252	4.815387
291.456634	7999.825407	9.656371	-0.059267	4.815376
291.661304	7999.834120	9.661376	-0.059305	4.815377
291.536231	7999.823501	9.666381	-0.059281	4.815375
291.706340	7999.878663	9.671386	-0.059313	4.815390
291.634638	7999.889227	9.676391	-0.059300	4.815394
291.780013	7999.930089	9.681395	-0.059327	4.815405
291.755139	7999.989515	9.686400	-0.059322	4.815422
291.596871	7999.867210	9.691405	-0.059292	4.815387
291.802892	7999.953955	9.696410	-0.059331	4.815412
291.578619	7999.842317	9.701415	-0.059289	4.815380
291.588654	7999.890563	9.706419	-0.059291	4.815394
291.713899	7999.889417	9.711424	-0.059314	4.815393
291.547787	7999.904835	9.716429	-0.059283	4.815399
291.509403	7999.954419	9.721434	-0.059276	4.815413
291.609032	7999.929341	9.726439	-0.059294	4.815405
291.612817	7999.899475	9.731443	-0.059295	4.815397
291.592516	7999.924779	9.736448	-0.059291	4.815404
291.545281	7999.905826	9.741453	-0.059282	4.815399
291.752174	7999.990449	9.746458	-0.059320	4.815423
291.851215	7999.968567	9.751463	-0.059339	4.815416
291.657611	7999.971776	9.756467	-0.059303	4.815418
291.581987	7999.980138	9.761472	-0.059288	4.815420
291.703613	7999.905198	9.766477	-0.059311	4.815398
291.602659	7999.927034	9.771482	-0.059292	4.815405
291.750793	7999.876041	9.776487	-0.059320	4.815389
291.697323	7999.916827	9.781491	-0.059310	4.815401
291.791050	7999.968592	9.786496	-0.059327	4.815416
291.744765	7999.895155	9.791501	-0.059318	4.815395
291.992709	7999.875730	9.796506	-0.059364	4.815388
292.016737	7999.870776	9.801511	-0.059369	4.815386
291.921236	7999.854232	9.806515	-0.059351	4.815382
291.904674	7999.881736	9.811520	-0.059348	4.815390
291.984730	7999.834962	9.816525	-0.059362	4.815376
292.076817	7999.965779	9.821530	-0.059380	4.815414
291.885919	7999.944454	9.826535	-0.059344	4.815409
291.794939	7999.908749	9.831539	-0.059327	4.815399
291.906723	7999.973636	9.836544	-0.059348	4.815417
291.660411	7999.901172	9.841549	-0.059302	4.815397
291.947369	7999.955057	9.846554	-0.059355	4.815411
292.020407	7999.907099	9.851559	-0.059369	4.815397
291.977592	7999.897836	9.856563	-0.059361	4.815395
292.008338	7999.964591	9.861568	-0.059366	4.815414
292.114991	7999.856276	9.866573	-0.059386	4.815382
292.067827	7999.914265	9.871578	-0.059377	4.815399
291.960703	7999.895391	9.876583	-0.059357	4.815394
292.157596	7999.872987	9.881587	-0.059394	4.815386
292.120578	7999.921526	9.886592	-0.059387	4.815401
292.209290	7999.924052	9.891597	-0.059403	4.815401
291.994347	7999.916222	9.896602	-0.059363	4.815400
292.114872	7999.923547	9.901607	-0.059385	4.815401
291.992823	7999.864889	9.906611	-0.059363	4.815385
292.073249	7999.884375	9.911616	-0.059377	4.815390
291.963179	7999.891101	9.916621	-0.059357	4.815393
291.966961	7999.899705	9.921626	-0.059358	4.815395
291.972221	7999.852765	9.926631	-0.059358	4.815381
292.199899	7999.889643	9.931635	-0.059401	4.815391
292.351120	7999.929534	9.936640	-0.059429	4.815402
292.185090	7999.846639	9.941645	-0.059398	4.815379
292.278158	7999.891982	9.946650	-0.059415	4.815391
292.409129	7999.886656	9.951655	-0.059439	4.815389
292.419209	7999.862237	9.956659	-0.059441	4.815382
292.278938	7999.867395	9.961664	-0.059415	4.815384
292.204612	7999.819141	9.966669	-0.059401	4.815370
292.264900	7999.888522	9.971674	-0.059412	4.815390
291.918247	7999.913783	9.976679	-0.059348	4.815399
292.221062	7999.913431	9.981683	-0.059404	4.815398
292.346917	7999.925119	9.986688	-0.059427	4.815401
292.232670	7999.845216	9.991693	-0.059406	4.815378
292.161668	7999.955175	9.996698	-0.059393	4.815410
292.228962	7999.939180	10.001703	-0.059405	4.815405
292.116231	7999.935175	10.006707	-0.059384	4.815405
292.092405	7999.979657	10.011712	-0.059379	4.815418
292.172300	7999.896547	10.016717	-0.059394	4.815393
292.161351	7999.907045	10.021722	-0.059392	4.815396
292.114019	7999.900914	10.026727	-0.059383	4.815395
292.173327	7999.936082	10.031731	-0.059394	4.815405
292.158104	7999.940098	10.036736	-0.059391	4.815406
292.120615	7999.921305	10.041741	-0.059384	4.815401
292.143876	7999.948398	10.046746	-0.059388	4.815409
292.304138	7999.927526	10.051751	-0.059418	4.815402
292.243670	7999.886981	10.056755	-0.059407	4.815390
292.224144	7999.915505	10.061760	-0.059403	4.815399
292.280177	7999.890776	10.066765	-0.059414	4.815391
292.368986	7999.955284	10.071770	-0.059430	4.815409
292.371338	7999.930737	10.076775	-0.059430	4.815402
292.483646	7999.943270	10.081779	-0.059451	4.815405
292.476328	7999.919632	10.086784	-0.059450	4.815399
292.426162	7999.854679	10.091789	-0.059440	4.815380
292.348610	7999.919647	10.096794	-0.059426	4.815399
292.390759	7999.879727	10.101799	-0.059434	4.815387
292.188211	7999.848593	10.106803	-0.059396	4.815379
292.294321	7999.955063	10.111808	-0.059415	4.815410
292.282474	7999.907840	10.116813	-0.059413	4.815396
292.350057	7999.959175	10.121818	-0.059426	4.815411
292.402280	7999.937588	10.126823	-0.059435	4.815404
292.418894	7999.887629	10.131827	-0.059438	4.815390
292.304423	7999.871841	10.136832	-0.059417	4.815385
292.252181	7999.891275	10.141837	-0.059407	4.815391
292.287444	7999.850173	10.146842	-0.059414	4.815379
292.422494	7999.981701	10.151847	-0.059439	4.815417
292.418117	7999.918571	10.156851	-0.059438	4.815399
292.440143	8000.006557	10.161856	-0.059442	4.815424
292.364874	7999.890962	10.166861	-0.059428	4.815391
292.667662	7999.883130	10.171866	-0.059484	4.815387
292.486127	7999.903636	10.176871	-0.059450	4.815394
292.462638	7999.941712	10.181875	-0.059446	4.815405
292.597756	7999.949279	10.186880	-0.059471	4.815407
292.372409	7999.875022	10.191885	-0.059429	4.815386
292.504023	7999.917795	10.196890	-0.059453	4.815398
292.429903	7999.878094	10.201895	-0.059439	4.815387
292.534445	7999.886224	10.206899	-0.059459	4.815389
292.484404	7999.920656	10.211904	-0.059449	4.815399
292.390710	7999.836817	10.216909	-0.059432	4.815375
292.443136	7999.899656	10.221914	-0.059441	4.815393
292.441847	7999.942373	10.226919	-0.059441	4.815405
292.413305	7999.911973	10.231923	-0.059436	4.815397
292.574732	7999.932798	10.236928	-0.059466	4.815402
292.672358	7999.866009	10.241933	-0.059484	4.815382
292.631440	7999.883494	10.246938	-0.059476	4.815387
292.407773	7999.927883	10.251943	-0.059434	4.815401
292.468761	7999.894686	10.256947	-0.059446	4.815391
292.625600	7999.909023	10.261952	-0.059475	4.815395
292.410563	7999.860583	10.266957	-0.059435	4.815382
292.476446	7999.895860	10.271962	-0.059447	4.815392
292.402846	7999.887158	10.276967	-0.059433	4.815390
292.359047	7999.859712	10.281971	-0.059425	4.815382
292.500347	7999.934704	10.286976	-0.059451	4.815403
292.653192	7999.877377	10.291981	-0.059479	4.815385
292.753715	7999.978413	10.296986	-0.059498	4.815414
292.572221	7999.942281	10.301991	-0.059464	4.815405
292.627401	7999.906851	10.306995	-0.059474	4.815394
292.660460	7999.956548	10.312000	-0.059480	4.815409
292.777408	7999.953128	10.317005	-0.059502	4.815407
292.852168	7999.929776	10.322010	-0.059516	4.815400
292.600351	7999.918131	10.327015	-0.059469	4.815398
292.774827	7999.900700	10.332019	-0.059501	4.815392
292.935996	8000.010220	10.337024	-0.059531	4.815423
292.913531	7999.905113	10.342029	-0.059527	4.815392
292.706792	7999.971155	10.347034	-0.059488	4.815413
292.635052	7999.955002	10.352039	-0.059475	4.815408
292.647808	7999.959481	10.357043	-0.059477	4.815409
292.642009	7999.980751	10.362048	-0.059476	4.815416
292.665561	7999.946936	10.367053	-0.059480	4.815406
292.831771	7999.911201	10.372058	-0.059511	4.815395
292.729014	7999.969342	10.377063	-0.059492	4.815412
292.654328	7999.956347	10.382067	-0.059478	4.815409
292.692443	7999.968724	10.387072	-0.059485	4.815412
292.765197	7999.874808	10.392077	-0.059499	4.815384
292.825807	7999.957019	10.397082	-0.059510	4.815408
292.594633	7999.945715	10.402087	-0.059467	4.815406
292.707333	7999.905891	10.407091	-0.059488	4.815394
292.799552	7999.984349	10.412096	-0.059505	4.815416
292.856161	7999.922226	10.417101	-0.059515	4.815398
293.007113	7999.919368	10.422106	-0.059543	4.815396
292.959156	7999.919638	10.427111	-0.059534	4.815396
292.907153	7999.848241	10.432115	-0.059524	4.815376
293.039172	7999.917739	10.437120	-0.059549	4.815395
293.118883	7999.916911	10.442125	-0.059564	4.815395
293.045350	7999.874012	10.447130	-0.059550	4.815383
292.994407	7999.911635	10.452135	-0.059540	4.815394
293.073100	7999.857357	10.457139	-0.059555	4.815378
293.069479	7999.937439	10.462144	-0.059554	4.815401
292.945720	7999.888368	10.467149	-0.059531	4.815387
292.945175	7999.927892	10.472154	-0.059531	4.815399
292.887862	7999.891673	10.477159	-0.059520	4.815389
292.780232	7999.867448	10.482163	-0.059500	4.815382
292.909875	7999.934768	10.487168	-0.059524	4.815401
293.079033	7999.902289	10.492173	-0.059555	4.815391
293.033969	7999.951764	10.497178	-0.059547	4.815405
292.954085	7999.949369	10.502183	-0.059532	4.815405
292.927456	7999.941442	10.507187	-0.059527	4.815403
293.056062	7999.983099	10.512192	-0.059551	4.815414
292.895504	7999.946243	10.517197	-0.059521	4.815404
293.089134	8000.025308	10.522202	-0.059557	4.815427
293.216355	8000.020990	10.527207	-0.059581	4.815425
293.076967	7999.923571	10.532211	-0.059554	4.815397
293.147940	7999.979237	10.537216	-0.059568	4.815413
292.932431	7999.945749	10.542221	-0.059527	4.815404
292.961519	7999.909888	10.547226	-0.059533	4.815394
293.008989	7999.943793	10.552231	-0.059541	4.815403
293.130967	7999.903053	10.557235	-0.059564	4.815391
293.192206	7999.955353	10.562240	-0.059575	4.815406
293.122266	7999.941367	10.567245	-0.059562	4.815402
292.997983	7999.974573	10.572250	-0.059539	4.815412
292.987992	7999.973333	10.577255	-0.059537	4.815412
293.136919	7999.927695	10.582259	-0.059565	4.815398
292.998156	7999.928603	10.587264	-0.059539	4.815399
293.015886	7999.926751	10.592269	-0.059542	4.815398
293.006962	7999.912704	10.597274	-0.059540	4.815394
293.086464	7999.919353	10.602279	-0.059555	4.815396
293.008407	7999.934087	10.607283	-0.059540	4.815400
293.210150	8000.007942	10.612288	-0.059578	4.815421
293.032893	7999.936614	10.617293	-0.059545	4.815401
293.059159	7999.988336	10.622298	-0.059550	4.815416
292.981790	7999.956060	10.627303	-0.059535	4.815407
293.092751	7999.919414	10.632307	-0.059556	4.815396
293.243328	7999.963571	10.637312	-0.059584	4.815408
293.175428	7999.950687	10.642317	-0.059571	4.815404
293.251602	7999.979723	10.647322	-0.059585	4.815413
293.146263	7999.959809	10.652327	-0.059565	4.815407
292.901515	7999.934388	10.657331	-0.059520	4.815401
293.217844	7999.965252	10.662336	-0.059579	4.815409
292.975233	7999.980474	10.667341	-0.059533	4.815414
293.236570	7999.944173	10.672346	-0.059582	4.815402
293.229282	7999.964350	10.677351	-0.059580	4.815408
293.191022	7999.948750	10.682355	-0.059573	4.815404
293.079960	7999.999273	10.687360	-0.059553	4.815419
293.066366	7999.927442	10.692365	-0.059550	4.815398
293.187090	7999.990342	10.697370	-0.059572	4.815416
293.097450	7999.990992	10.702375	-0.059556	4.815417
293.087306	7999.988680	10.707379	-0.059554	4.815416
293.319973	7999.985034	10.712384	-0.059597	4.815414
293.350199	7999.960947	10.717389	-0.059602	4.815407
293.436957	7999.982677	10.722394	-0.059618	4.815413
293.225251	7999.940702	10.727399	-0.059579	4.815401
293.295782	7999.927967	10.732403	-0.059592	4.815397
293.172898	7999.980432	10.737408	-0.059569	4.815413
293.202873	7999.945654	10.742413	-0.059574	4.815403
293.380003	7999.978495	10.747418	-0.059607	4.815412
293.122235	7999.945377	10.752423	-0.059559	4.815403
293.118356	7999.904697	10.757427	-0.059558	4.815391
293.141321	7999.971326	10.762432	-0.059563	4.815411
293.041704	7999.880975	10.767437	-0.059544	4.815385
293.156867	7999.953401	10.772442	-0.059565	4.815405
293.178653	7999.930243	10.777447	-0.059569	4.815399
293.183449	7999.888638	10.782451	-0.059570	4.815386
293.342099	7999.991705	10.787456	-0.059600	4.815416
293.157327	7999.956586	10.792461	-0.059565	4.815406
293.275783	7999.971359	10.797466	-0.059587	4.815410
293.123649	7999.982732	10.802471	-0.059559	4.815414
293.123793	7999.915402	10.807475	-0.059559	4.815395
293.068347	7999.981805	10.812480	-0.059548	4.815414
293.163593	7999.973752	10.817485	-0.059566	4.815411
293.332770	7999.988294	10.822490	-0.059597	4.815415
293.241828	7999.979305	10.827495	-0.059580	4.815413
293.298467	7999.931075	10.832499	-0.059591	4.815398
293.322286	7999.941079	10.837504	-0.059595	4.815401
293.105438	7999.908637	10.842509	-0.059555	4.815393
293.176223	7999.987811	10.847514	-0.059568	4.815415
293.274868	8000.011875	10.852519	-0.059586	4.815422
293.160082	7999.981118	10.857523	-0.059565	4.815414
293.300959	8000.019772	10.862528	-0.059591	4.815424
293.192555	7999.947443	10.867533	-0.059571	4.815404
293.127027	8000.005130	10.872538	-0.059558	4.815421
293.323490	8000.008367	10.877543	-0.059595	4.815421
293.341066	7999.990483	10.882547	-0.059598	4.815415
293.281317	8000.014069	10.887552	-0.059587	4.815423
293.043946	7999.984494	10.892557	-0.059543	4.815415
293.153690	8000.018359	10.897562	-0.059563	4.815424
293.419320	7999.968236	10.902567	-0.059612	4.815409
293.239963	7999.868019	10.907571	-0.059579	4.815380
293.411165	7999.932821	10.912576	-0.059611	4.815398
293.370318	7999.885119	10.917581	-0.059603	4.815385
293.433791	7999.965241	10.922586	-0.059615	4.815408
293.410616	7999.883633	10.927591	-0.059610	4.815384
293.488377	7999.863536	10.932595	-0.059625	4.815378
293.418887	7999.960699	10.937600	-0.059612	4.815406
293.212806	7999.965837	10.942605	-0.059573	4.815409
293.574095	7999.965385	10.947610	-0.059640	4.815407
293.415973	7999.958492	10.952615	-0.059611	4.815406
293.336363	7999.900531	10.957619	-0.059596	4.815389
293.510506	7999.910880	10.962624	-0.059628	4.815391
293.463810	7999.872699	10.967629	-0.059619	4.815380
293.366079	7999.887108	10.972634	-0.059601	4.815385
293.311925	7999.958875	10.977639	-0.059591	4.815406
293.682170	7999.892313	10.982643	-0.059660	4.815385
293.394991	7999.976263	10.987648	-0.059606	4.815411
293.238388	7999.969395	10.992653	-0.059577	4.815410
293.251949	8000.020907	10.997658	-0.059580	4.815425
293.583901	7999.996460	11.002663	-0.059641	4.815416
293.220654	7999.927403	11.007667	-0.059574	4.815398
293.397107	7999.989086	11.012672	-0.059606	4.815415
293.458364	7999.961236	11.017677	-0.059618	4.815406
293.761646	7999.954483	11.022682	-0.059674	4.815403
293.607439	7999.981852	11.027687	-0.059645	4.815412
293.452939	7999.898074	11.032691	-0.059616	4.815388
293.552160	7999.989474	11.037696	-0.059635	4.815414
293.545114	7999.925230	11.042701	-0.059633	4.815395
293.454812	7999.950448	11.047706	-0.059616	4.815403
293.476602	7999.963625	11.052711	-0.059620	4.815407
293.455586	7999.878846	11.057715	-0.059616	4.815382
293.630796	7999.973638	11.062720	-0.059649	4.815409
293.459067	7999.879958	11.067725	-0.059617	4.815383
293.385452	7999.927894	11.072730	-0.059603	4.815397
293.484833	7999.920979	11.077735	-0.059622	4.815395
293.549107	7999.899591	11.082739	-0.059633	4.815388
293.655112	7999.946219	11.087744	-0.059653	4.815401
293.441400	7999.960849	11.092749	-0.059613	4.815406
293.509772	7999.921362	11.097754	-0.059626	4.815395
293.760526	7999.959694	11.102759	-0.059673	4.815404
293.686185	7999.893270	11.107763	-0.059659	4.815385
293.489539	7999.949860	11.112768	-0.059622	4.815403
293.483560	7999.887772	11.117773	-0.059621	4.815385
293.633804	7999.847499	11.122778	-0.059649	4.815372
293.414093	7999.914396	11.127783	-0.059608	4.815393
293.429076	7999.903949	11.132787	-0.059610	4.815390
293.686177	7999.955210	11.137792	-0.059658	4.815404
293.521603	7999.920424	11.142797	-0.059627	4.815394
293.767541	7999.905243	11.147802	-0.059673	4.815389
293.833113	7999.954409	11.152807	-0.059685	4.815403
293.688703	7999.929575	11.157811	-0.059658	4.815396
293.560004	7999.959502	11.162816	-0.059634	4.815405
293.478387	7999.920744	11.167821	-0.059619	4.815395
293.548866	7999.900527	11.172826	-0.059632	4.815388
293.523330	7999.939639	11.177831	-0.059627	4.815400
293.470526	7999.924867	11.182835	-0.059617	4.815396
293.602609	7999.998642	11.187840	-0.059642	4.815417
293.515955	7999.946976	11.192845	-0.059626	4.815402
293.459982	7999.969555	11.197850	-0.059615	4.815409
293.667956	7999.977258	11.202855	-0.059654	4.815410
293.640747	7999.932986	11.207859	-0.059649	4.815397
293.604526	7999.985814	11.212864	-0.059642	4.815413
293.505380	7999.962796	11.217869	-0.059623	4.815407
293.538981	7999.887469	11.222874	-0.059629	4.815385
293.375440	7999.954224	11.227879	-0.059599	4.815405
293.399614	7999.915075	11.232883	-0.059603	4.815393
293.674855	7999.978391	11.237888	-0.059654	4.815410
293.615895	7999.970998	11.242893	-0.059643	4.815409
293.572272	7999.975613	11.247898	-0.059635	4.815410
293.681451	7999.968860	11.252903	-0.059655	4.815408
293.642864	7999.904096	11.257907	-0.059648	4.815389
293.834896	7999.885886	11.262912	-0.059684	4.815383
293.757326	7999.888873	11.267917	-0.059669	4.815384
293.713145	7999.925539	11.272922	-0.059661	4.815395
293.760783	7999.926319	11.277927	-0.059670	4.815395
293.538314	7999.898059	11.282931	-0.059628	4.815388
293.826070	7999.978680	11.287936	-0.059682	4.815410
293.552195	7999.936745	11.292941	-0.059631	4.815399
293.571185	7999.911404	11.297946	-0.059634	4.815391
293.654632	7999.981170	11.302951	-0.059650	4.815411
293.613658	7999.939876	11.307955	-0.059642	4.815399
293.752327	7999.980632	11.312960	-0.059668	4.815411
293.689483	7999.930428	11.317965	-0.059656	4.815396
293.628027	7999.947573	11.322970	-0.059644	4.815402
293.681792	8000.016849	11.327975	-0.059654	4.815422
293.650473	7999.978921	11.332979	-0.059648	4.815411
293.805927	7999.999649	11.337984	-0.059677	4.815416
293.712429	8000.002372	11.342989	-0.059660	4.815417
293.755973	7999.982779	11.347994	-0.059668	4.815411
294.015174	7999.950719	11.352999	-0.059716	4.815401
293.727755	7999.901080	11.358003	-0.059662	4.815388
293.738116	7999.991012	11.363008	-0.059664	4.815414
293.653311	7999.957544	11.368013	-0.059648	4.815404
293.758261	7999.946447	11.373018	-0.059668	4.815401
293.527945	7999.982176	11.378023	-0.059625	4.815412
293.406071	7999.880771	11.383027	-0.059602	4.815383
293.712041	7999.996958	11.388032	-0.059659	4.815416
293.718689	7999.987443	11.393037	-0.059660	4.815413
293.488526	7999.986840	11.398042	-0.059617	4.815414
293.581425	7999.990505	11.403047	-0.059634	4.815414
293.567703	7999.999889	11.408051	-0.059632	4.815417
293.471840	8000.019672	11.413056	-0.059614	4.815424
293.616504	7999.979307	11.418061	-0.059641	4.815411
293.642650	7999.967977	11.423066	-0.059645	4.815408
293.512342	7999.978641	11.428071	-0.059621	4.815411
293.473662	7999.933111	11.433075	-0.059614	4.815398
293.535630	7999.926647	11.438080	-0.059625	4.815396
293.498710	7999.895039	11.443085	-0.059618	4.815387
293.545892	7999.906497	11.448090	-0.059627	4.815390
293.605465	7999.955564	11.453095	-0.059638	4.815404
293.746784	7999.905526	11.458099	-0.059664	4.815389
293.727658	7999.961843	11.463104	-0.059661	4.815405
293.517229	7999.929506	11.468109	-0.059621	4.815397
293.677499	7999.906498	11.473114	-0.059651	4.815390
293.804870	7999.941723	11.478119	-0.059675	4.815399
293.637081	7999.957112	11.483123	-0.059643	4.815404
293.712211	8000.014986	11.488128	-0.059657	4.815421
293.756583	7999.991132	11.493133	-0.059666	4.815414
293.651828	7999.999012	11.498138	-0.059646	4.815417
293.721116	8000.004425	11.503143	-0.059659	4.815418
293.853315	7999.992708	11.508147	-0.059683	4.815414
293.780830	7999.979748	11.513152	-0.059670	4.815410
293.838943	7999.944366	11.518157	-0.059680	4.815400
293.634154	7999.954869	11.523162	-0.059642	4.815404
293.825156	7999.991146	11.528167	-0.059678	4.815414
293.605550	7999.915911	11.533171	-0.059637	4.815393
293.651475	7999.972233	11.538176	-0.059645	4.815409
293.805398	7999.913854	11.543181	-0.059674	4.815391
293.761284	7999.946247	11.548186	-0.059666	4.815401
293.748019	7999.982355	11.553191	-0.059663	4.815411
293.713879	7999.912321	11.558195	-0.059656	4.815391
293.700581	7999.965527	11.563200	-0.059654	4.815407
293.765090	7999.914221	11.568205	-0.059666	4.815391
293.887906	7999.918380	11.573210	-0.059689	4.815392
293.817712	7999.947136	11.578215	-0.059676	4.815401
293.832241	7999.864012	11.583219	-0.059678	4.815376
293.770864	7999.993369	11.588224	-0.059667	4.815414
293.995193	7999.999205	11.593229	-0.059708	4.815415
294.003645	7999.923462	11.598234	-0.059710	4.815393
293.940913	7999.968371	11.603239	-0.059698	4.815406
293.975888	7999.934744	11.608243	-0.059704	4.815396
294.060079	7999.978875	11.613248	-0.059720	4.815409
293.967370	7999.935658	11.618253	-0.059703	4.815397
293.866578	7999.963909	11.623258	-0.059684	4.815405
293.990524	7999.967018	11.628263	-0.059707	4.815406
293.972682	7999.956029	11.633267	-0.059704	4.815403
293.876818	7999.975812	11.638272	-0.059686	4.815409
293.763938	7999.954704	11.643277	-0.059664	4.815403
293.952471	7999.925751	11.648282	-0.059699	4.815394
293.950931	7999.987702	11.653287	-0.059699	4.815412
293.927307	7999.907154	11.658291	-0.059695	4.815389
293.809707	7999.976805	11.663296	-0.059673	4.815409
293.853970	7999.916615	11.668301	-0.059681	4.815392
293.948655	7999.941682	11.673306	-0.059698	4.815399
293.944263	8000.002517	11.678311	-0.059698	4.815416
293.826903	7999.936451	11.683315	-0.059676	4.815398
293.897846	7999.993187	11.688320	-0.059689	4.815414
293.881449	7999.973673	11.693325	-0.059686	4.815408
294.094296	7999.914129	11.698330	-0.059725	4.815390
294.035303	7999.961238	11.703335	-0.059714	4.815404
293.883392	7999.856129	11.708339	-0.059686	4.815374
294.026826	7999.957878	11.713344	-0.059712	4.815403
293.977230	7999.947434	11.718349	-0.059703	4.815400
293.971460	7999.922752	11.723354	-0.059702	4.815393
293.909522	7999.965537	11.728359	-0.059690	4.815406
293.797514	7999.957268	11.733363	-0.059669	4.815404
293.905948	8000.013554	11.738368	-0.059689	4.815420
293.779430	7999.959092	11.743373	-0.059666	4.815404
293.834296	8000.013425	11.748378	-0.059676	4.815420
293.867575	8000.022517	11.753383	-0.059682	4.815423
293.822061	7999.990766	11.758387	-0.059673	4.815414
293.958571	8000.042174	11.763392	-0.059699	4.815428
293.803978	8000.007552	11.768397	-0.059670	4.815419
293.864030	7999.994644	11.773402	-0.059681	4.815414
293.797036	7999.999943	11.778407	-0.059668	4.815416
293.923531	7999.948591	11.783411	-0.059692	4.815401
293.814483	7999.962813	11.788416	-0.059672	4.815405
293.852324	7999.948469	11.793421	-0.059679	4.815401
293.801897	7999.913432	11.798426	-0.059669	4.815391
293.841654	7999.950416	11.803431	-0.059676	4.815402
293.735095	7999.934756	11.808435	-0.059656	4.815398
294.071726	8000.040765	11.813440	-0.059719	4.815427
293.973373	8000.038065	11.818445	-0.059701	4.815427
293.952552	8000.017409	11.823450	-0.059697	4.815421
294.132085	8000.037466	11.828455	-0.059730	4.815426
294.129175	7999.951917	11.833459	-0.059729	4.815401
294.030284	7999.990886	11.838464	-0.059711	4.815413
293.817373	7999.926447	11.843469	-0.059671	4.815395
294.047850	7999.874676	11.848474	-0.059714	4.815379
294.145626	7999.974602	11.853479	-0.059732	4.815407
294.005269	7999.922049	11.858483	-0.059706	4.815393
294.196657	7999.975431	11.863488	-0.059742	4.815407
293.987380	7999.950593	11.868493	-0.059702	4.815401
293.893983	7999.991790	11.873498	-0.059685	4.815414
293.918370	7999.988980	11.878503	-0.059689	4.815413
293.836365	7999.896781	11.883507	-0.059674	4.815386
293.935492	7999.977493	11.888512	-0.059692	4.815409
293.985978	7999.950534	11.893517	-0.059702	4.815401
294.045417	7999.963264	11.898522	-0.059713	4.815404
293.997419	7999.967808	11.903527	-0.059704	4.815406
293.889935	7999.901905	11.908531	-0.059684	4.815387
294.198326	7999.977524	11.913536	-0.059741	4.815408
294.111792	7999.921585	11.918541	-0.059725	4.815392
294.019472	7999.924328	11.923546	-0.059708	4.815393
293.950910	7999.958454	11.928551	-0.059695	4.815404
294.016957	7999.886868	11.933555	-0.059707	4.815382
294.086863	7999.940381	11.938560	-0.059720	4.815398
294.020235	7999.915762	11.943565	-0.059707	4.815391
294.071149	7999.983923	11.948570	-0.059717	4.815410
294.115337	8000.012432	11.953575	-0.059725	4.815419
293.883976	7999.904941	11.958579	-0.059682	4.815388
294.086521	7999.914691	11.963584	-0.059719	4.815390
294.022314	7999.916830	11.968589	-0.059707	4.815391
294.009895	7999.876008	11.973594	-0.059705	4.815379
294.120586	7999.953705	11.978599	-0.059725	4.815401
294.043213	7999.922497	11.983603	-0.059711	4.815393
294.222203	7999.970331	11.988608	-0.059744	4.815406
294.247481	7999.930131	11.993613	-0.059749	4.815394
294.243688	7999.939680	11.998618	-0.059748	4.815397
294.253585	7999.945180	12.003623	-0.059750	4.815398
294.230825	7999.917011	12.008627	-0.059746	4.815390
294.298834	7999.951256	12.013632	-0.059758	4.815400
294.203550	7999.992422	12.018637	-0.059740	4.815412
294.145137	7999.911299	12.023642	-0.059729	4.815389
294.024304	7999.954181	12.028647	-0.059707	4.815402
294.120830	7999.887373	12.033651	-0.059725	4.815382
294.145625	7999.925179	12.038656	-0.059729	4.815393
293.988262	7999.903336	12.043661	-0.059700	4.815387
294.175628	7999.841235	12.048666	-0.059735	4.815368
294.237581	7999.936294	12.053671	-0.059746	4.815396
294.124196	7999.864950	12.058675	-0.059725	4.815375
294.169750	7999.922335	12.063680	-0.059733	4.815392
294.090113	7999.909257	12.068685	-0.059718	4.815389
294.010391	7999.853431	12.073690	-0.059703	4.815373
294.130198	7999.938760	12.078695	-0.059726	4.815397
294.132138	7999.904587	12.083699	-0.059726	4.815387
294.130445	7999.928063	12.088704	-0.059726	4.815394
294.130971	7999.916309	12.093709	-0.059726	4.815390
294.110374	7999.898862	12.098714	-0.059722	4.815385
294.138010	7999.955952	12.103719	-0.059727	4.815402
293.794774	7999.873331	12.108723	-0.059663	4.815380
293.957791	7999.956167	12.113728	-0.059693	4.815403
294.118252	7999.923544	12.118733	-0.059723	4.815393
294.250813	7999.927864	12.123738	-0.059747	4.815393
294.010287	7999.998691	12.128743	-0.059703	4.815415
293.970889	7999.933912	12.133747	-0.059695	4.815396
294.159119	7999.946632	12.138752	-0.059730	4.815399
294.018099	7999.933609	12.143757	-0.059704	4.815396
294.035877	7999.925346	12.148762	-0.059707	4.815394
294.085283	7999.975314	12.153767	-0.059716	4.815408
294.023935	7999.901624	12.158771	-0.059705	4.815387
294.019124	7999.992375	12.163776	-0.059704	4.815413
293.864883	7999.872266	12.168781	-0.059675	4.815379
293.969713	7999.895363	12.173786	-0.059694	4.815385
294.196856	7999.965366	12.178791	-0.059736	4.815404
294.274498	7999.897177	12.183795	-0.059751	4.815384
294.268246	7999.875693	12.188800	-0.059750	4.815378
293.988245	7999.959761	12.193805	-0.059697	4.815404
294.164772	7999.835498	12.198810	-0.059730	4.815367
294.310208	7999.874228	12.203815	-0.059757	4.815377
294.057391	7999.856152	12.208819	-0.059710	4.815373
294.125194	7999.896806	12.213824	-0.059723	4.815385
294.189760	7999.934200	12.218829	-0.059734	4.815395
294.108013	7999.865516	12.223834	-0.059719	4.815376
294.070220	7999.910838	12.228839	-0.059712	4.815389
294.236871	7999.853737	12.233843	-0.059743	4.815372
294.322480	7999.934227	12.238848	-0.059759	4.815395
294.122076	7999.926634	12.243853	-0.059721	4.815394
294.262572	7999.857347	12.248858	-0.059748	4.815373
294.341609	7999.921697	12.253863	-0.059762	4.815391
294.277002	7999.851159	12.258867	-0.059750	4.815371
294.404493	7999.941958	12.263872	-0.059774	4.815397
294.467184	7999.953673	12.268877	-0.059785	4.815400
294.396199	7999.916158	12.273882	-0.059772	4.815389
294.314048	7999.970365	12.278887	-0.059757	4.815405
294.437489	7999.975604	12.283891	-0.059780	4.815406
294.410467	7999.967669	12.288896	-0.059774	4.815404
294.238498	7999.994744	12.293901	-0.059742	4.815413
294.387006	7999.941619	12.298906	-0.059770	4.815397
294.407815	7999.987909	12.303911	-0.059774	4.815410
294.282922	7999.948435	12.308915	-0.059750	4.815399
294.293930	7999.943266	12.313920	-0.059752	4.815398
294.131411	7999.935231	12.318925	-0.059722	4.815396
294.241780	7999.910330	12.323930	-0.059742	4.815388
294.322453	7999.911655	12.328935	-0.059757	4.815388
294.293623	7999.926134	12.333939	-0.059752	4.815393
294.347089	7999.983650	12.338944	-0.059762	4.815409
294.202787	7999.980190	12.343949	-0.059735	4.815409
294.129329	7999.893475	12.348954	-0.059721	4.815384
294.286055	7999.909950	12.353959	-0.059750	4.815388
294.013913	7999.889417	12.358963	-0.059699	4.815383
294.208243	7999.903307	12.363968	-0.059736	4.815386
294.417281	7999.929195	12.368973	-0.059774	4.815393
294.369432	7999.890994	12.373978	-0.059765	4.815382
294.292546	7999.967730	12.378983	-0.059751	4.815405
294.250379	7999.930691	12.383987	-0.059743	4.815394
294.182785	7999.957353	12.388992	-0.059730	4.815402
294.125929	7999.917934	12.393997	-0.059720	4.815391
294.196838	7999.902000	12.399002	-0.059733	4.815386
294.281328	7999.957891	12.404007	-0.059749	4.815402
294.073185	7999.878570	12.409011	-0.059710	4.815380
294.076529	7999.892510	12.414016	-0.059710	4.815384
294.229815	7999.911065	12.419021	-0.059739	4.815389
294.324253	7999.857047	12.424026	-0.059756	4.815372
294.300764	7999.977413	12.429031	-0.059752	4.815408
294.211161	7999.915010	12.434035	-0.059735	4.815390
294.427399	7999.889721	12.439040	-0.059775	4.815381
294.363604	7999.901484	12.444045	-0.059763	4.815385
294.362925	7999.837345	12.449050	-0.059763	4.815366
294.297584	7999.946333	12.454055	-0.059751	4.815399
294.230488	7999.920637	12.459059	-0.059738	4.815391
294.286009	7999.870251	12.464064	-0.059748	4.815376
294.353089	7999.892725	12.469069	-0.059761	4.815383
294.383730	7999.884675	12.474074	-0.059766	4.815380
294.217277	7999.915047	12.479079	-0.059735	4.815390
294.249378	7999.909158	12.484083	-0.059741	4.815388
294.361184	7999.900311	12.489088	-0.059762	4.815385
294.187048	7999.932694	12.494093	-0.059730	4.815395
294.367677	7999.864069	12.499098	-0.059763	4.815374
294.462646	7999.942576	12.504103	-0.059781	4.815397
294.319377	7999.876081	12.509107	-0.059754	4.815378
294.324315	7999.913559	12.514112	-0.059755	4.815389
294.387440	7999.958411	12.519117	-0.059766	4.815402
294.428743	7999.935575	12.524122	-0.059774	4.815395
294.157664	7999.955670	12.529127	-0.059724	4.815402
294.189042	7999.834352	12.534131	-0.059729	4.815366
294.275557	7999.962946	12.539136	-0.059745	4.815404
294.162546	7999.926874	12.544141	-0.059724	4.815394
294.156271	7999.889360	12.549146	-0.059723	4.815383
294.216638	7999.951265	12.554151	-0.059734	4.815400
294.080252	7999.872060	12.559155	-0.059709	4.815378
294.235440	7999.893852	12.564160	-0.059737	4.815384
294.172352	7999.913108	12.569165	-0.059726	4.815390
294.251749	7999.927236	12.574170	-0.059740	4.815393
294.388659	7999.931628	12.579175	-0.059766	4.815394
294.302810	7999.889593	12.584179	-0.059750	4.815382
294.244940	7999.990155	12.589184	-0.059739	4.815412
294.351241	7999.982286	12.594189	-0.059759	4.815409
294.136458	7999.906060	12.599194	-0.059718	4.815388
294.287159	7999.959839	12.604199	-0.059746	4.815403
294.279137	7999.882754	12.609203	-0.059745	4.815380
294.222457	7999.905322	12.614208	-0.059734	4.815387
294.137921	7999.937047	12.619213	-0.059718	4.815397
294.181601	7999.878985	12.624218	-0.059726	4.815380
294.274579	7999.942497	12.629223	-0.059744	4.815398
294.080818	7999.870894	12.634227	-0.059707	4.815378
294.073982	7999.926345	12.639232	-0.059706	4.815394
294.137852	7999.900676	12.644237	-0.059718	4.815386
294.373385	7999.916315	12.649242	-0.059762	4.815390
294.302383	7999.973912	12.654247	-0.059748	4.815407
294.284170	7999.956505	12.659251	-0.059745	4.815402
294.294939	7999.944920	12.664256	-0.059747	4.815398
294.135488	7999.928386	12.669261	-0.059717	4.815394
294.068272	7999.847119	12.674266	-0.059704	4.815371
294.095920	7999.998251	12.679271	-0.059710	4.815415
294.128813	7999.952834	12.684275	-0.059716	4.815401
294.072877	7999.934804	12.689280	-0.059705	4.815396
294.069152	7999.977483	12.694285	-0.059704	4.815409
294.310864	7999.859639	12.699290	-0.059749	4.815373
294.461277	7999.958298	12.704295	-0.059777	4.815401
294.299925	7999.931046	12.709299	-0.059747	4.815394
294.321771	7999.935674	12.714304	-0.059751	4.815395
294.038585	7999.971599	12.719309	-0.059698	4.815407
294.215561	7999.913600	12.724314	-0.059731	4.815390
294.346839	8000.015149	12.729319	-0.059756	4.815419
294.277057	7999.971242	12.734323	-0.059742	4.815406
294.378867	7999.966505	12.739328	-0.059761	4.815404
294.272120	7999.981833	12.744333	-0.059741	4.815409
294.360297	7999.942673	12.749338	-0.059758	4.815397
294.299922	7999.980141	12.754343	-0.059746	4.815409
294.313767	7999.905555	12.759347	-0.059749	4.815387
294.594520	7999.943315	12.764352	-0.059801	4.815396
294.540942	7999.970208	12.769357	-0.059791	4.815404
294.335321	7999.971079	12.774362	-0.059753	4.815406
294.357205	7999.927617	12.779367	-0.059757	4.815393
294.173421	7999.894651	12.784371	-0.059722	4.815384
294.248600	7999.938633	12.789376	-0.059736	4.815397
294.453368	7999.927047	12.794381	-0.059774	4.815392
294.211397	7999.901669	12.799386	-0.059729	4.815386
294.219733	7999.993706	12.804391	-0.059731	4.815413
294.184788	7999.914039	12.809395	-0.059724	4.815390
294.295299	7999.983185	12.814400	-0.059745	4.815409
294.113125	7999.954520	12.819405	-0.059711	4.815402
294.190471	7999.963271	12.824410	-0.059725	4.815404
294.376837	7999.887260	12.829415	-0.059759	4.815381
294.472330	7999.861045	12.834419	-0.059777	4.815373
294.555499	7999.882716	12.839424	-0.059793	4.815379
294.613399	7999.915726	12.844429	-0.059803	4.815388
294.682153	7999.842047	12.849434	-0.059816	4.815366
294.567989	7999.918168	12.854439	-0.059795	4.815389
294.404066	7999.847057	12.859443	-0.059764	4.815369
294.510236	7999.876590	12.864448	-0.059784	4.815377
294.225894	7999.936006	12.869453	-0.059731	4.815396
294.314029	7999.878678	12.874458	-0.059747	4.815379
294.599000	7999.961392	12.879463	-0.059800	4.815402
294.477389	7999.904873	12.884467	-0.059777	4.815386
294.499553	7999.938361	12.889472	-0.059781	4.815395
294.573564	7999.956676	12.894477	-0.059795	4.815400
294.312668	7999.926710	12.899482	-0.059746	4.815393
294.229986	7999.968084	12.904487	-0.059731	4.815405
294.274294	7999.895070	12.909491	-0.059739	4.815384
294.306880	7999.884915	12.914496	-0.059745	4.815381
294.352753	7999.956198	12.919501	-0.059754	4.815401
294.144905	7999.882225	12.924506	-0.059715	4.815381
294.494152	7999.976688	12.929511	-0.059780	4.815407
294.469952	7999.888648	12.934515	-0.059775	4.815381
294.363665	7999.892229	12.939520	-0.059755	4.815383
294.422344	7999.972274	12.944525	-0.059766	4.815406
294.332981	7999.916287	12.949530	-0.059749	4.815390
294.356680	7999.967969	12.954535	-0.059754	4.815405
294.315751	7999.936293	12.959539	-0.059746	4.815396
294.410477	7999.979530	12.964544	-0.059764	4.815408
294.309707	7999.963965	12.969549	-0.059745	4.815404
294.475467	7999.936773	12.974554	-0.059776	4.815395
294.495716	8000.008703	12.979559	-0.059779	4.815416
294.406004	7999.872559	12.984563	-0.059762	4.815377
294.267889	7999.890576	12.989568	-0.059737	4.815383
294.282812	7999.927150	12.994573	-0.059739	4.815393
294.317457	7999.852908	12.999578	-0.059746	4.815371
294.434312	7999.928570	13.004583	-0.059767	4.815393
294.395347	7999.867004	13.009587	-0.059760	4.815375
294.488022	7999.927305	13.014592	-0.059777	4.815392
294.409056	7999.902483	13.019597	-0.059762	4.815385
294.310748	7999.879478	13.024602	-0.059744	4.815379
294.472066	7999.923814	13.029607	-0.059774	4.815391
294.416044	7999.855555	13.034611	-0.059763	4.815372
294.386182	7999.910626	13.039616	-0.059758	4.815388
294.295543	7999.882404	13.044621	-0.059741	4.815380
294.440828	7999.866630	13.049626	-0.059768	4.815375
294.452263	7999.911696	13.054631	-0.059770	4.815388
294.323620	7999.925594	13.059635	-0.059746	4.815393
294.514301	7999.941561	13.064640	-0.059781	4.815396
294.388973	7999.958720	13.069645	-0.059758	4.815402
294.277934	7999.898101	13.074650	-0.059737	4.815385
294.381672	7999.926524	13.079655	-0.059756	4.815393
294.415725	7999.878989	13.084659	-0.059763	4.815379
294.546730	7999.886489	13.089664	-0.059787	4.815380
294.354417	7999.887580	13.094669	-0.059751	4.815381
294.371548	7999.892131	13.099674	-0.059754	4.815383
294.566544	7999.962672	13.104679	-0.059790	4.815402
294.284679	7999.920605	13.109683	-0.059738	4.815391
294.397634	7999.867961	13.114688	-0.059759	4.815375
294.374908	7999.904982	13.119693	-0.059754	4.815386
294.379076	7999.885807	13.124698	-0.059755	4.815381
294.412179	7999.907721	13.129703	-0.059761	4.815387
294.357100	7999.891842	13.134707	-0.059751	4.815383
294.425288	7999.867313	13.139712	-0.059764	4.815375
294.420410	7999.977300	13.144717	-0.059763	4.815407
294.295419	7999.920725	13.149722	-0.059739	4.815391
294.509610	7999.941355	13.154727	-0.059779	4.815396
294.544394	7999.857496	13.159731	-0.059785	4.815372
294.529647	7999.935260	13.164736	-0.059783	4.815395
294.511992	7999.938167	13.169741	-0.059779	4.815395
294.419074	7999.932350	13.174746	-0.059762	4.815394
294.464939	7999.960886	13.179751	-0.059770	4.815402
294.483686	7999.900274	13.184755	-0.059774	4.815385
294.509578	7999.864359	13.189760	-0.059778	4.815374
294.456617	7999.886988	13.194765	-0.059768	4.815381
294.597573	7999.873279	13.199770	-0.059795	4.815376
294.675993	7999.919453	13.204775	-0.059809	4.815389
294.611876	7999.880982	13.209779	-0.059797	4.815378
294.572436	7999.857881	13.214784	-0.059790	4.815372
294.524719	7999.909451	13.219789	-0.059781	4.815387
294.526828	7999.857113	13.224794	-0.059781	4.815372
294.662241	7999.892472	13.229799	-0.059806	4.815381
294.629194	7999.899400	13.234803	-0.059800	4.815384
294.467647	7999.927716	13.239808	-0.059770	4.815393
294.346156	7999.979136	13.244813	-0.059747	4.815408
294.466404	7999.871041	13.249818	-0.059769	4.815376
294.600874	7999.921346	13.254823	-0.059794	4.815390
294.404359	7999.873208	13.259827	-0.059758	4.815377
294.659387	7999.940466	13.264832	-0.059805	4.815395
294.720378	7999.906200	13.269837	-0.059816	4.815385
294.762841	7999.843842	13.274842	-0.059824	4.815367
294.676562	7999.917217	13.279847	-0.059808	4.815389
294.673619	7999.863727	13.284851	-0.059807	4.815373
294.659931	7999.885937	13.289856	-0.059805	4.815380
294.561609	7999.919572	13.294861	-0.059786	4.815390
294.591976	7999.892280	13.299866	-0.059792	4.815382
294.728250	7999.943684	13.304871	-0.059817	4.815396
294.692138	7999.913157	13.309875	-0.059810	4.815387
294.789049	7999.938262	13.314880	-0.059828	4.815394
294.604603	8000.004673	13.319885	-0.059794	4.815414
294.562944	7999.971917	13.324890	-0.059786	4.815405
294.434941	7999.990100	13.329895	-0.059762	4.815411
294.766130	7999.944267	13.334899	-0.059824	4.815396
294.765765	7999.939979	13.339904	-0.059824	4.815395
294.543637	7999.934165	13.344909	-0.059782	4.815394
294.545850	7999.866867	13.349914	-0.059783	4.815375
294.661582	7999.896558	13.354919	-0.059804	4.815383
294.689397	7999.842507	13.359923	-0.059809	4.815367
294.661088	7999.940352	13.364928	-0.059804	4.815395
294.739284	7999.923469	13.369933	-0.059818	4.815390
294.752575	7999.894826	13.374938	-0.059821	4.815382
294.515473	7999.975329	13.379943	-0.059777	4.815406
294.369723	7999.906655	13.384947	-0.059749	4.815387
294.427882	7999.895853	13.389952	-0.059760	4.815384
294.520542	7999.937987	13.394957	-0.059777	4.815395
294.434595	7999.923736	13.399962	-0.059761	4.815392
294.429298	7999.936465	13.404967	-0.059760	4.815395
294.327390	7999.871723	13.409971	-0.059741	4.815377
294.445704	7999.889700	13.414976	-0.059763	4.815382
294.501595	7999.913058	13.419981	-0.059773	4.815388
294.410208	7999.919022	13.424986	-0.059756	4.815390
294.405079	7999.965953	13.429991	-0.059755	4.815404
294.363483	7999.900069	13.434995	-0.059747	4.815385
294.521519	7999.856719	13.440000	-0.059777	4.815372
294.597619	7999.929571	13.445005	-0.059791	4.815393
294.386434	7999.941036	13.450010	-0.059751	4.815397
294.622383	8000.002636	13.455015	-0.059795	4.815414
294.386400	7999.958120	13.460019	-0.059751	4.815402
294.199910	7999.934728	13.465024	-0.059716	4.815396
294.424568	7999.973698	13.470029	-0.059758	4.815406
294.522920	7999.916538	13.475034	-0.059776	4.815389
294.346322	7999.963842	13.480039	-0.059743	4.815404
294.303439	7999.854121	13.485043	-0.059735	4.815372
294.616725	7999.915929	13.490048	-0.059794	4.815389
294.302766	7999.874400	13.495053	-0.059735	4.815378
294.394284	7999.913309	13.500058	-0.059752	4.815389
294.739755	7999.941451	13.505063	-0.059816	4.815395
294.573923	7999.876721	13.510067	-0.059785	4.815377
294.525828	7999.909048	13.515072	-0.059776	4.815387
294.507514	7999.942937	13.520077	-0.059773	4.815397
294.590347	7999.911169	13.525082	-0.059788	4.815387
294.500201	7999.921428	13.530087	-0.059771	4.815391
294.362692	7999.900981	13.535091	-0.059746	4.815385
294.495594	7999.905307	13.540096	-0.059770	4.815386
294.642130	7999.899171	13.545101	-0.059797	4.815384
294.536517	7999.904900	13.550106	-0.059778	4.815386
294.527118	7999.906875	13.555111	-0.059776	4.815386
294.439375	7999.866946	13.560115	-0.059759	4.815375
294.747430	7999.934012	13.565120	-0.059817	4.815393
294.695026	7999.947032	13.570125	-0.059807	4.815397
294.578666	7999.917316	13.575130	-0.059785	4.815389
294.386798	7999.955818	13.580135	-0.059749	4.815401
294.496553	7999.904190	13.585139	-0.059770	4.815386
294.500429	7999.901041	13.590144	-0.059770	4.815385
294.725585	7999.917578	13.595149	-0.059812	4.815389
294.541834	7999.822628	13.600154	-0.059778	4.815362
294.767047	7999.920386	13.605159	-0.059820	4.815389
294.754425	7999.862461	13.610163	-0.059817	4.815372
294.781207	7999.856484	13.615168	-0.059822	4.815370
294.753299	7999.974640	13.620173	-0.059817	4.815405
294.698542	7999.926706	13.625178	-0.059807	4.815391
294.728763	7999.956053	13.630183	-0.059812	4.815400
294.554919	7999.979891	13.635187	-0.059780	4.815408
294.823805	7999.897762	13.640192	-0.059830	4.815382
294.585828	7999.966494	13.645197	-0.059785	4.815404
294.473048	7999.961418	13.650202	-0.059764	4.815403
294.567355	8000.004648	13.655207	-0.059782	4.815415
294.698767	7999.880706	13.660211	-0.059806	4.815378
294.446935	7999.918218	13.665216	-0.059759	4.815390
294.552496	7999.964839	13.670221	-0.059779	4.815403
294.542804	7999.922993	13.675226	-0.059777	4.815391
294.713546	8000.021989	13.680231	-0.059809	4.815419
294.590520	7999.905600	13.685235	-0.059786	4.815386
294.527982	7999.977230	13.690240	-0.059774	4.815407
294.513460	7999.975914	13.695245	-0.059771	4.815407
294.449107	7999.870113	13.700250	-0.059759	4.815376
294.613674	7999.929465	13.705255	-0.059790	4.815393
294.512107	7999.894650	13.710259	-0.059771	4.815383
294.689128	7999.928559	13.715264	-0.059803	4.815392
294.586782	7999.906556	13.720269	-0.059784	4.815386
294.629784	7999.824971	13.725274	-0.059792	4.815362
294.638109	7999.912734	13.730279	-0.059794	4.815388
294.488748	7999.925221	13.735283	-0.059766	4.815392
294.555043	7999.902798	13.740288	-0.059778	4.815385
294.585878	7999.891544	13.745293	-0.059784	4.815382
294.638509	7999.888132	13.750298	-0.059793	4.815380
294.853565	7999.961143	13.755303	-0.059833	4.815401
294.660810	7999.946195	13.760307	-0.059797	4.815397
294.683461	7999.878166	13.765312	-0.059802	4.815377
294.612369	7999.998815	13.770317	-0.059788	4.815413
294.414236	7999.978435	13.775322	-0.059751	4.815408
294.587897	7999.977023	13.780327	-0.059784	4.815407
294.515303	7999.860398	13.785331	-0.059770	4.815373
294.632031	7999.860182	13.790336	-0.059792	4.815372
294.838984	7999.890311	13.795341	-0.059830	4.815380
294.641746	7999.861397	13.800346	-0.059793	4.815373
294.572895	7999.970327	13.805351	-0.059780	4.815405
294.730478	7999.921626	13.810355	-0.059810	4.815390
294.810305	7999.872709	13.815360	-0.059824	4.815375
294.630436	7999.926371	13.820365	-0.059791	4.815392
294.700788	7999.935007	13.825370	-0.059804	4.815394
294.693544	7999.964804	13.830375	-0.059802	4.815403
294.596367	7999.910825	13.835379	-0.059784	4.815387
294.792759	7999.882002	13.840384	-0.059821	4.815378
294.948272	7999.960442	13.845389	-0.059850	4.815400
294.854160	7999.884071	13.850394	-0.059832	4.815378
294.782353	7999.946999	13.855399	-0.059819	4.815397
294.761236	7999.995803	13.860403	-0.059815	4.815411
294.745153	8000.021178	13.865408	-0.059811	4.815419
294.686635	7999.977457	13.870413	-0.059800	4.815406
294.696644	7999.876090	13.875418	-0.059802	4.815377
294.720560	7999.963041	13.880423	-0.059807	4.815402
294.605097	7999.871357	13.885427	-0.059785	4.815376
294.812450	7999.884393	13.890432	-0.059824	4.815379
294.709136	7999.929702	13.895437	-0.059804	4.815392
294.505543	7999.897477	13.900442	-0.059766	4.815384
294.577916	7999.935000	13.905447	-0.059780	4.815395
294.720477	7999.866815	13.910451	-0.059806	4.815374
294.649036	7999.922268	13.915456	-0.059793	4.815390
294.682903	7999.958087	13.920461	-0.059799	4.815401
294.868154	7999.886332	13.925466	-0.059833	4.815379
294.919935	7999.953440	13.930471	-0.059843	4.815398
294.699154	7999.832229	13.935475	-0.059802	4.815364
294.663663	7999.863696	13.940480	-0.059795	4.815373
294.853476	7999.903160	13.945485	-0.059830	4.815384
294.872055	7999.853232	13.950490	-0.059834	4.815369
294.749347	7999.877915	13.955495	-0.059811	4.815377
294.796185	7999.860514	13.960499	-0.059819	4.815372
294.952503	7999.851333	13.965504	-0.059848	4.815368
294.842205	7999.930724	13.970509	-0.059828	4.815392
294.646977	7999.859096	13.975514	-0.059791	4.815372
294.998551	7999.932225	13.980519	-0.059857	4.815392
294.876910	7999.899216	13.985523	-0.059834	4.815383
294.964663	7999.891040	13.990528	-0.059850	4.815380
294.889698	7999.950710	13.995533	-0.059836	4.815398
295.008247	7999.901364	14.000538	-0.059858	4.815383
294.976944	7999.948931	14.005543	-0.059852	4.815397
294.863394	7999.954529	14.010547	-0.059831	4.815399
295.053214	7999.954452	14.015552	-0.059866	4.815398
294.803399	7999.984515	14.020557	-0.059820	4.815408
294.757381	7999.917489	14.025562	-0.059811	4.815389
294.932942	7999.971680	14.030567	-0.059844	4.815404
294.833336	7999.900562	14.035571	-0.059825	4.815383
294.701819	7999.912275	14.040576	-0.059801	4.815387
294.732823	7999.957665	14.045581	-0.059806	4.815400
294.911925	7999.883671	14.050586	-0.059839	4.815378
294.869068	7999.938528	14.055591	-0.059831	4.815394
294.851354	7999.891205	14.060595	-0.059828	4.815380
294.889277	7999.995488	14.065600	-0.059835	4.815411
294.857899	7999.997100	14.070605	-0.059829	4.815411
294.698849	7999.948511	14.075610	-0.059799	4.815398
294.796337	8000.018511	14.080615	-0.059818	4.815418
294.767825	7999.912232	14.085619	-0.059812	4.815387
294.944079	7999.888420	14.090624	-0.059845	4.815379
294.841015	7999.981824	14.095629	-0.059826	4.815407
294.868108	7999.909593	14.100634	-0.059831	4.815386
294.805387	7999.951297	14.105639	-0.059819	4.815398
294.790243	7999.910430	14.110643	-0.059816	4.815386
294.868233	7999.899955	14.115648	-0.059830	4.815383
294.845728	7999.941255	14.120653	-0.059826	4.815395
294.634920	7999.889674	14.125658	-0.059787	4.815381
295.065661	7999.926707	14.130663	-0.059867	4.815390
294.928613	7999.961840	14.135667	-0.059841	4.815401
294.754660	7999.926898	14.140672	-0.059809	4.815391
294.789403	7999.959525	14.145677	-0.059815	4.815401
294.753930	7999.880918	14.150682	-0.059808	4.815378
294.734737	7999.896624	14.155687	-0.059805	4.815383
294.667608	7999.865585	14.160691	-0.059792	4.815374
294.795401	7999.854865	14.165696	-0.059816	4.815370
294.811945	7999.967343	14.170701	-0.059819	4.815403
294.661180	7999.871869	14.175706	-0.059791	4.815376
294.994652	7999.959661	14.180711	-0.059853	4.815400
294.951111	7999.880920	14.185715	-0.059845	4.815377
294.849559	7999.849311	14.190720	-0.059826	4.815368
294.904679	7999.853421	14.195725	-0.059836	4.815369
294.769284	7999.827666	14.200730	-0.059810	4.815362
294.823663	7999.886266	14.205735	-0.059821	4.815379
294.787835	7999.909178	14.210739	-0.059814	4.815386
294.827765	7999.919449	14.215744	-0.059821	4.815389
294.939668	7999.972588	14.220749	-0.059842	4.815404
294.761071	7999.849937	14.225754	-0.059809	4.815369
294.840625	7999.916434	14.230759	-0.059823	4.815388
294.791489	7999.871799	14.235763	-0.059814	4.815375
294.770983	7999.858629	14.240768	-0.059810	4.815371
294.872984	7999.896642	14.245773	-0.059829	4.815382
294.984782	7999.934818	14.250778	-0.059850	4.815393
294.775423	7999.970893	14.255783	-0.059811	4.815404
294.694548	7999.997336	14.260787	-0.059796	4.815412
294.765153	7999.851016	14.265792	-0.059809	4.815369
294.905128	7999.608594	14.270797	-0.059834	4.815298
294.897046	7996.389929	14.275802	-0.059831	4.814357
295.029031	7990.780398	14.280807	-0.059852	4.812717
294.962711	7983.945966	14.285811	-0.059835	4.810720
295.023549	7976.694889	14.290816	-0.059841	4.808599
294.712927	7969.030458	14.295821	-0.059778	4.806357
294.676007	7961.236453	14.300826	-0.059766	4.804076
294.723599	7953.368616	14.305831	-0.059770	4.801771
294.587277	7945.373935	14.310835	-0.059739	4.799429
294.534249	7937.429180	14.315840	-0.059724	4.797100
294.704938	7929.391602	14.320845	-0.059751	4.794742
294.699612	7921.380875	14.325850	-0.059744	4.792391
294.605378	7913.337726	14.330855	-0.059721	4.790029
294.660346	7905.420777	14.335859	-0.059726	4.787704
294.573729	7897.356995	14.340864	-0.059705	4.785334
294.559024	7889.451096	14.345869	-0.059697	4.783009
294.532388	7881.368530	14.350874	-0.059687	4.780632
294.352590	7873.422617	14.355879	-0.059648	4.778294
294.098397	7865.376874	14.360883	-0.059595	4.775925
294.214440	7857.405746	14.365888	-0.059612	4.773576
294.506007	7849.361355	14.370893	-0.059661	4.771204
294.334001	7841.314982	14.375898	-0.059623	4.768831
294.246513	7833.425008	14.380903	-0.059602	4.766504
294.236283	7825.363315	14.385907	-0.059595	4.764124
294.064991	7817.442148	14.390912	-0.059557	4.761785
294.090225	7809.360404	14.395917	-0.059557	4.759396
293.954377	7801.372674	14.400922	-0.059526	4.757035
294.008200	7793.348950	14.405927	-0.059531	4.754662
293.880411	7785.296579	14.410931	-0.059502	4.752279
293.801636	7777.282582	14.415936	-0.059482	4.749906
294.011990	7769.320040	14.420941	-0.059516	4.747547
293.874176	7761.325000	14.425946	-0.059485	4.745177
293.712787	7753.351658	14.430951	-0.059449	4.742813
293.750758	7745.343400	14.435955	-0.059451	4.740437
293.605612	7737.309952	14.440960	-0.059419	4.738053
293.613598	7729.335737	14.445965	-0.059415	4.735684
293.673386	7721.329258	14.450970	-0.059421	4.733305
293.834684	7713.287869	14.455975	-0.059446	4.730914
293.630517	7705.313170	14.460979	-0.059402	4.728543
293.628409	7697.296171	14.465984	-0.059397	4.726157
293.635013	7689.312660	14.470989	-0.059393	4.723780
293.332020	7681.302159	14.475994	-0.059331	4.721394
293.606943	7673.357357	14.480999	-0.059377	4.719025
293.689449	7665.312254	14.486003	-0.059387	4.716626
293.582360	7657.318830	14.491008	-0.059362	4.714242
293.544968	7649.263141	14.496013	-0.059349	4.711837
293.327574	7641.242574	14.501018	-0.059304	4.709442
293.459662	7633.328083	14.506023	-0.059323	4.707077
293.422879	7625.255490	14.511027	-0.059311	4.704664
293.321985	7617.303468	14.516032	-0.059287	4.702285
293.346537	7609.349101	14.521037	-0.059286	4.699905
293.192059	7601.309970	14.526042	-0.059252	4.697498
293.248977	7593.277481	14.531047	-0.059257	4.695092
293.176792	7585.304492	14.536051	-0.059238	4.692702
293.038997	7577.221741	14.541056	-0.059207	4.690278
293.034108	7569.303200	14.546061	-0.059201	4.687903
293.208637	7561.231702	14.551066	-0.059228	4.685479
293.271820	7553.295665	14.556071	-0.059235	4.683096
293.094283	7545.250149	14.561075	-0.059197	4.680678
293.135983	7537.336685	14.566080	-0.059199	4.678299
293.036335	7529.283325	14.571085	-0.059175	4.675877
293.168394	7521.182439	14.576090	-0.059194	4.673438
293.025385	7513.174612	14.581095	-0.059162	4.671027
292.920235	7505.226063	14.586099	-0.059138	4.668633
292.962814	7497.166313	14.591104	-0.059140	4.666203
292.986136	7489.226584	14.596109	-0.059139	4.663808
292.745598	7481.231960	14.601114	-0.059089	4.661396
292.799023	7473.246820	14.606119	-0.059094	4.658986
292.640740	7465.231978	14.611123	-0.059059	4.656565
292.457157	7457.229551	14.616128	-0.059020	4.654146
292.676553	7449.228518	14.621133	-0.059055	4.651727
292.608143	7441.164682	14.626138	-0.059037	4.649287
292.449602	7433.223443	14.631143	-0.059002	4.646884
292.415879	7425.167159	14.636147	-0.058991	4.644444
292.501065	7417.247263	14.641152	-0.059001	4.642044
292.672792	7409.175143	14.646157	-0.059028	4.639597
292.507768	7401.259861	14.651162	-0.058992	4.637196
292.628868	7393.236145	14.656167	-0.059009	4.634761
292.454912	7385.207902	14.661171	-0.058972	4.632323
292.317751	7377.146002	14.666176	-0.058941	4.629874
292.351222	7369.181056	14.671181	-0.058942	4.627453
292.351244	7361.139163	14.676186	-0.058936	4.625007
292.210388	7353.227576	14.681191	-0.058905	4.622600
292.178758	7345.186972	14.686195	-0.058894	4.620152
292.406109	7337.218399	14.691200	-0.058931	4.617724
292.351723	7329.175002	14.696205	-0.058915	4.615273
292.015756	7321.147143	14.701210	-0.058847	4.612825
292.064110	7313.173771	14.706215	-0.058851	4.610392
291.999871	7305.153507	14.711219	-0.058834	4.607944
292.121913	7297.107812	14.716224	-0.058851	4.605487
292.080910	7289.200284	14.721229	-0.058838	4.603070
291.857840	7281.184802	14.726234	-0.058792	4.600619
291.872544	7273.222404	14.731239	-0.058789	4.598184
291.850014	7265.186775	14.736243	-0.058780	4.595724
292.017275	7257.125630	14.741248	-0.058805	4.593256
291.856698	7249.099866	14.746253	-0.058770	4.590796
291.869641	7241.101568	14.751258	-0.058767	4.588344
292.100575	7233.112192	14.756263	-0.058805	4.585894
291.940149	7225.110591	14.761267	-0.058770	4.583438
291.540552	7217.110882	14.766272	-0.058690	4.580981
291.647523	7209.156966	14.771277	-0.058705	4.578538
291.812396	7201.126887	14.776282	-0.058730	4.576070
291.708346	7193.148576	14.781287	-0.058705	4.573616
291.533304	7185.071369	14.786291	-0.058668	4.571130
291.636179	7177.127442	14.791296	-0.058681	4.568684
291.854453	7169.095125	14.796301	-0.058717	4.566210
291.580043	7161.114518	14.801306	-0.058660	4.563750
291.506990	7153.127408	14.806311	-0.058641	4.561287
291.518121	7145.145310	14.811315	-0.058638	4.558824
291.308761	7137.157371	14.816320	-0.058594	4.556357
291.298870	7129.133532	14.821325	-0.058587	4.553879
291.262359	7121.072796	14.826330	-0.058575	4.551387
291.319474	7113.118982	14.831335	-0.058580	4.548928
291.243457	7105.095493	14.836339	-0.058561	4.546445
291.335345	7097.094684	14.841344	-0.058572	4.543969
291.536378	7089.122799	14.846349	-0.058605	4.541500
291.114217	7081.065083	14.851354	-0.058521	4.539002
291.164274	7073.106819	14.856359	-0.058525	4.536534
291.340050	7065.075648	14.861363	-0.058552	4.534043
291.116851	7057.104637	14.866368	-0.058505	4.531568
291.081151	7049.096661	14.871373	-0.058493	4.529081
291.037849	7041.090144	14.876378	-0.058480	4.526592
291.118972	7033.103259	14.881383	-0.058490	4.524109
290.753440	7025.153995	14.886387	-0.058416	4.521635
290.679649	7017.085787	14.891392	-0.058397	4.519124
291.072139	7009.143885	14.896397	-0.058465	4.516651
290.781764	7001.054171	14.901402	-0.058406	4.514129
290.497496	6993.068153	14.906407	-0.058348	4.511639
290.618069	6985.030381	14.911411	-0.058365	4.509131
290.585636	6977.017301	14.916416	-0.058353	4.506630
290.588493	6969.056361	14.921421	-0.058349	4.504144
290.525852	6961.073423	14.926426	-0.058332	4.501649
290.664241	6953.050245	14.931431	-0.058352	4.499141
290.500242	6945.089094	14.936435	-0.058316	4.496650
290.561045	6937.039620	14.941440	-0.058322	4.494130
290.547184	6929.072081	14.946445	-0.058315	4.491635
290.276508	6921.027785	14.951450	-0.058259	4.489113
290.345683	6913.071398	14.956455	-0.058266	4.486619
290.493497	6905.020139	14.961459	-0.058289	4.484093
290.393624	6897.068360	14.966464	-0.058265	4.481597
290.415362	6889.072096	14.971469	-0.058263	4.479085
290.338632	6881.065466	14.976474	-0.058244	4.476569
290.585771	6873.056914	14.981479	-0.058285	4.474052
290.353207	6865.014384	14.986483	-0.058236	4.471521
290.192431	6857.000495	14.991488	-0.058201	4.468998
290.435284	6849.049055	14.996493	-0.058241	4.466494
290.139463	6841.018075	15.001498	-0.058180	4.463962
290.162621	6833.050394	15.006503	-0.058179	4.461450
290.169521	6825.064640	15.011507	-0.058175	4.458930
290.172450	6817.023143	15.016512	-0.058171	4.456392
290.122498	6809.030364	15.021517	-0.058156	4.453867
289.950813	6800.974538	15.026522	-0.058119	4.451321
290.111677	6793.034655	15.031527	-0.058143	4.448810
290.090219	6784.992052	15.036531	-0.058134	4.446266
290.098915	6777.024660	15.041536	-0.058130	4.443743
289.988749	6769.012138	15.046541	-0.058105	4.441205
290.040235	6760.982375	15.051546	-0.058109	4.438660
290.014895	6752.993687	15.056551	-0.058099	4.436127
289.849118	6744.979067	15.061555	-0.058063	4.433583
289.926721	6736.949972	15.066560	-0.058072	4.431034
289.597537	6728.982359	15.071565	-0.058005	4.428502
289.565402	6720.936599	15.076570	-0.057994	4.425944
289.736946	6712.991647	15.081575	-0.058021	4.423418
289.719448	6704.993167	15.086579	-0.058012	4.420873
289.450066	6696.998192	15.091584	-0.057957	4.418326
289.605984	6688.959345	15.096589	-0.057980	4.415765
289.482753	6680.937242	15.101594	-0.057952	4.413207
289.367999	6672.970598	15.106599	-0.057925	4.410666
289.396183	6664.951575	15.111603	-0.057925	4.408107
289.413197	6656.935431	15.116608	-0.057923	4.405547
289.375805	6649.029347	15.121613	-0.057911	4.403021
289.335552	6640.937501	15.126618	-0.057898	4.400433
289.608659	6633.024770	15.131623	-0.057944	4.397904
289.261814	6624.961116	15.136627	-0.057874	4.395321
289.137706	6616.987254	15.141632	-0.057846	4.392766
289.317229	6608.970998	15.146637	-0.057874	4.390199
289.184796	6600.957967	15.151642	-0.057844	4.387629
289.186559	6592.950257	15.156647	-0.057839	4.385060
289.232956	6584.982429	15.161651	-0.057842	4.382502
289.262805	6576.959294	15.166656	-0.057842	4.379925
289.232183	6569.027431	15.171661	-0.057831	4.377376
289.185630	6560.939391	15.176666	-0.057817	4.374774
289.213347	6553.009038	15.181671	-0.057817	4.372223
289.098764	6544.926023	15.186675	-0.057791	4.369620
288.956816	6536.982092	15.191680	-0.057759	4.367060
288.978528	6528.971014	15.196685	-0.057758	4.364477
288.919341	6521.011717	15.201690	-0.057741	4.361910
288.782313	6513.009332	15.206695	-0.057711	4.359326
288.851587	6504.987400	15.211699	-0.057718	4.356736
288.844242	6496.932137	15.216704	-0.057711	4.354134
288.763778	6488.891856	15.221709	-0.057691	4.351534
288.802195	6480.890676	15.226714	-0.057693	4.348945
288.745896	6472.929935	15.231719	-0.057677	4.346368
288.709749	6464.922458	15.236723	-0.057665	4.343774
288.798167	6456.984605	15.241728	-0.057676	4.341203
288.604991	6448.968802	15.246733	-0.057635	4.338602
288.737493	6440.943284	15.251738	-0.057655	4.335999
288.492963	6432.973874	15.256743	-0.057604	4.333410
288.455919	6424.960655	15.261747	-0.057592	4.330806
288.574827	6416.942157	15.266752	-0.057608	4.328201
288.474358	6408.936152	15.271757	-0.057584	4.325596
288.356592	6400.946909	15.276762	-0.057557	4.322995
288.428316	6392.928578	15.281767	-0.057565	4.320384
288.288450	6384.973488	15.286771	-0.057534	4.317791
288.174543	6376.951813	15.291776	-0.057507	4.315175
288.177548	6368.911325	15.296781	-0.057503	4.312552
288.487778	6360.863841	15.301786	-0.057555	4.309927
288.404781	6352.933521	15.306791	-0.057534	4.307336
288.286333	6344.884706	15.311795	-0.057507	4.304705
288.102740	6336.975070	15.316800	-0.057468	4.302117
288.186148	6328.941803	15.321805	-0.057478	4.299489
287.989630	6320.944958	15.326810	-0.057436	4.296869
287.976145	6312.944816	15.331815	-0.057428	4.294247
288.002400	6304.885765	15.336819	-0.057428	4.291605
287.974087	6296.900574	15.341824	-0.057417	4.288986
287.984449	6288.913613	15.346829	-0.057414	4.286364
287.815425	6280.928441	15.351834	-0.057377	4.283740
287.899188	6272.920953	15.356839	-0.057387	4.281109
288.038796	6264.938769	15.361843	-0.057408	4.278486
287.921914	6256.913952	15.366848	-0.057381	4.275844
287.843569	6248.896944	15.371853	-0.057361	4.273204
287.599258	6240.879783	15.376858	-0.057310	4.270560
287.729311	6232.873011	15.381863	-0.057329	4.267922
287.795833	6224.873773	15.386867	-0.057336	4.265284
287.760144	6216.907718	15.391872	-0.057324	4.262654
287.764559	6208.898276	15.396877	-0.057320	4.260009
287.620309	6200.908221	15.401882	-0.057288	4.257367
287.637842	6192.923508	15.406887	-0.057286	4.254727
287.558755	6184.923763	15.411891	-0.057266	4.252079
287.549773	6176.864892	15.416896	-0.057259	4.249411
287.647011	6168.922128	15.421901	-0.057271	4.246780
287.586220	6160.874763	15.426906	-0.057255	4.244112
287.517225	6152.955975	15.431911	-0.057237	4.241484
287.368760	6144.897703	15.436915	-0.057204	4.238808
287.529700	6136.906221	15.441920	-0.057228	4.236155
287.460453	6128.916920	15.446925	-0.057210	4.233499
287.342872	6120.867436	15.451930	-0.057183	4.230821
287.280029	6112.919988	15.456935	-0.057166	4.228176
287.092180	6104.909042	15.461939	-0.057126	4.225507
287.058027	6096.938044	15.466944	-0.057114	4.222851
287.152311	6088.941116	15.471949	-0.057126	4.220185
286.983362	6080.949604	15.476954	-0.057090	4.217518
287.188903	6072.909872	15.481959	-0.057123	4.214836
287.014824	6064.909115	15.486963	-0.057085	4.212161
287.079879	6056.895016	15.491968	-0.057092	4.209483
287.151538	6048.977244	15.496973	-0.057100	4.206836
287.182983	6040.872639	15.501978	-0.057100	4.204124
287.136525	6032.959276	15.506983	-0.057086	4.201473
286.956144	6024.948016	15.511987	-0.057048	4.198787
286.780604	6016.930643	15.516992	-0.057010	4.196097
286.794117	6008.889250	15.521997	-0.057007	4.193398
286.886588	6000.796604	15.527002	-0.057019	4.190682
286.703853	5992.896358	15.532007	-0.056979	4.188026
286.909094	5984.822514	15.537011	-0.057012	4.185314
286.849279	5976.900665	15.542016	-0.056996	4.182649
286.589508	5968.944067	15.547021	-0.056942	4.179967
286.324516	5960.915028	15.552026	-0.056888	4.177260
286.532307	5952.913658	15.557031	-0.056921	4.174565
286.407314	5944.900673	15.562035	-0.056892	4.171861
286.528436	5936.863448	15.567040	-0.056910	4.169150
286.361134	5928.939988	15.572045	-0.056873	4.166472
286.343078	5920.883661	15.577050	-0.056865	4.163750
286.337382	5912.933723	15.582055	-0.056858	4.161061
286.427856	5904.902632	15.587059	-0.056870	4.158345
286.395525	5896.897574	15.592064	-0.056858	4.155634
286.358352	5888.884111	15.597069	-0.056846	4.152919
286.197657	5880.854433	15.602074	-0.056811	4.150194
286.413470	5872.881331	15.607079	-0.056846	4.147492
286.340608	5864.847190	15.612083	-0.056827	4.144764
286.209922	5856.889325	15.617088	-0.056797	4.142059
286.298790	5848.890354	15.622093	-0.056809	4.139341
286.207712	5840.881019	15.627098	-0.056786	4.136615
286.317728	5832.902791	15.632103	-0.056802	4.133901
286.074981	5824.880201	15.637107	-0.056751	4.131165
286.139971	5816.847276	15.642112	-0.056758	4.128428
286.129179	5808.863605	15.647117	-0.056751	4.125705
286.109089	5800.902020	15.652122	-0.056742	4.122988
286.100845	5792.901396	15.657127	-0.056735	4.120256
286.012843	5784.919094	15.662131	-0.056713	4.117527
285.904044	5776.882669	15.667136	-0.056687	4.114777
285.945792	5768.843288	15.672141	-0.056690	4.112027
285.868683	5760.817401	15.677146	-0.056670	4.109277
285.901641	5752.849228	15.682151	-0.056671	4.106547
285.859096	5744.888310	15.687155	-0.056658	4.103817
285.711807	5736.905796	15.692160	-0.056625	4.101076
285.581270	5728.905318	15.697165	-0.056596	4.098328
285.423782	5720.894959	15.702170	-0.056561	4.095574
285.537660	5712.891323	15.707175	-0.056577	4.092823
285.527913	5704.848866	15.712179	-0.056570	4.090056
285.332929	5696.885306	15.717184	-0.056528	4.087312
285.418130	5688.893490	15.722189	-0.056539	4.084560
285.408938	5680.946985	15.727194	-0.056532	4.081821
285.311486	5672.932439	15.732199	-0.056508	4.079055
285.233588	5664.959663	15.737203	-0.056489	4.076301
285.341207	5656.925227	15.742208	-0.056503	4.073527
285.413035	5648.922049	15.747213	-0.056511	4.070762
285.294803	5640.901324	15.752218	-0.056484	4.067986
285.308297	5632.895186	15.757223	-0.056481	4.065215
285.277998	5624.961177	15.762227	-0.056470	4.062466
285.336070	5616.891157	15.767232	-0.056476	4.059670
285.374233	5608.977769	15.772237	-0.056478	4.056925
285.210983	5600.907252	15.777242	-0.056442	4.054122
285.240213	5592.918823	15.782247	-0.056442	4.051348
285.129938	5584.930037	15.787251	-0.056416	4.048569
285.080572	5576.911920	15.792256	-0.056402	4.045780
285.102333	5568.968982	15.797261	-0.056401	4.043016
285.110511	5560.917355	15.802266	-0.056397	4.040211
285.294750	5552.953348	15.807271	-0.056426	4.037439
285.265980	5544.934084	15.812275	-0.056415	4.034641
284.935072	5536.852943	15.817280	-0.056348	4.031816
284.897317	5528.840877	15.822285	-0.056336	4.029017
285.053402	5520.859012	15.827290	-0.056360	4.026230
284.977242	5512.899006	15.832295	-0.056340	4.023444
284.724878	5504.899671	15.837299	-0.056288	4.020641
284.761840	5496.910209	15.842304	-0.056290	4.017843
285.038722	5488.921920	15.847309	-0.056336	4.015048
284.798959	5480.885524	15.852314	-0.056286	4.012226
284.738153	5472.894918	15.857319	-0.056269	4.009420
284.692865	5464.909243	15.862323	-0.056256	4.006615
284.638508	5456.894964	15.867328	-0.056240	4.003797
284.750774	5448.940049	15.872333	-0.056256	4.001001
284.505843	5440.912885	15.877338	-0.056205	3.998172
284.459003	5432.951593	15.882343	-0.056191	3.995367
284.300539	5424.913370	15.887347	-0.056156	3.992531
284.390330	5416.867744	15.892352	-0.056167	3.989695
284.432368	5408.917550	15.897357	-0.056170	3.986890
284.313128	5400.907969	15.902362	-0.056142	3.984059
284.434237	5392.926495	15.907367	-0.056160	3.981239
284.290782	5384.963889	15.912371	-0.056128	3.978420
284.202503	5376.970897	15.917376	-0.056106	3.975590
284.048900	5368.928573	15.922381	-0.056072	3.972738
284.303685	5360.876278	15.927386	-0.056114	3.969888
284.216068	5352.940964	15.932391	-0.056093	3.967072
284.188100	5344.917048	15.937395	-0.056082	3.964223
284.321203	5336.944789	15.942400	-0.056102	3.961393
284.341932	5328.989732	15.947405	-0.056100	3.958566
284.103579	5320.969534	15.952410	-0.056051	3.955709
284.147983	5312.957300	15.957415	-0.056054	3.952857
284.052566	5304.922608	15.962419	-0.056030	3.949993
284.058885	5296.908073	15.967424	-0.056026	3.947136
283.944230	5288.950772	15.972429	-0.056000	3.944295
283.799772	5280.952653	15.977434	-0.055967	3.941436
283.864479	5272.963155	15.982439	-0.055974	3.938583
283.875781	5264.962006	15.987443	-0.055971	3.935722
283.848658	5256.973826	15.992448	-0.055961	3.932863
283.747818	5248.983833	15.997453	-0.055937	3.930000
283.504814	5240.982471	16.002458	-0.055886	3.927129
283.517591	5232.994183	16.007463	-0.055883	3.924264
283.683865	5225.005696	16.012467	-0.055909	3.921401
283.761918	5216.975326	16.017472	-0.055918	3.918518
283.644044	5209.032043	16.022477	-0.055891	3.915661
283.541857	5200.985345	16.027482	-0.055867	3.912765
283.619841	5192.922386	16.032487	-0.055876	3.909864
283.477000	5184.979019	16.037491	-0.055844	3.907001
283.572062	5176.969481	16.042496	-0.055856	3.904115
283.427749	5169.027591	16.047501	-0.055824	3.901248
283.402723	5161.001524	16.052506	-0.055814	3.898350
283.392237	5152.997959	16.057511	-0.055807	3.895458
283.243415	5144.981725	16.062515	-0.055774	3.892557
283.165039	5136.943668	16.067520	-0.055754	3.889648
283.204459	5128.985587	16.072525	-0.055756	3.886767
283.202973	5120.977864	16.077530	-0.055750	3.883865
283.410145	5113.026106	16.082535	-0.055784	3.880986
283.190033	5105.041127	16.087539	-0.055738	3.878084
283.241177	5096.974603	16.092544	-0.055742	3.875156
283.210181	5088.782917	16.097549	-0.055731	3.872178
282.861441	5080.863585	16.102554	-0.055660	3.869291
283.037849	5072.884066	16.107559	-0.055688	3.866390
282.984919	5064.940962	16.112563	-0.055673	3.863495
282.803205	5056.958662	16.117568	-0.055634	3.860582
282.817388	5048.980273	16.122573	-0.055631	3.857671
282.758125	5040.923051	16.127578	-0.055615	3.854729
282.868363	5032.978809	16.132583	-0.055630	3.851828
282.687984	5024.996888	16.137587	-0.055591	3.848906
282.559389	5016.995202	16.142592	-0.055562	3.845975
282.901642	5009.020244	16.147597	-0.055620	3.843062
282.698228	5001.002588	16.152602	-0.055577	3.840120
282.709528	4993.047167	16.157607	-0.055574	3.837202
282.786164	4985.054998	16.162611	-0.055583	3.834270
282.651170	4977.002739	16.167616	-0.055552	3.831310
282.632085	4969.023190	16.172621	-0.055544	3.828376
282.579027	4960.989786	16.177626	-0.055528	3.825419
282.756249	4953.046923	16.182631	-0.055556	3.822499
282.625225	4945.043060	16.187635	-0.055526	3.819547
282.375689	4937.074280	16.192640	-0.055475	3.816603
282.585006	4929.078475	16.197645	-0.055508	3.813657
282.480875	4921.025821	16.202650	-0.055484	3.810681
282.479595	4913.086669	16.207655	-0.055478	3.807746
282.453367	4905.059763	16.212659	-0.055468	3.804777
282.397110	4897.109187	16.217664	-0.055452	3.801832
282.244298	4889.087921	16.222669	-0.055419	3.798857
282.090602	4881.079798	16.227674	-0.055385	3.795885
282.190622	4873.075627	16.232679	-0.055398	3.792917
282.014799	4865.057079	16.237683	-0.055360	3.789936
282.089274	4857.045975	16.242688	-0.055368	3.786960
282.143858	4849.066663	16.247693	-0.055373	3.783993
282.006662	4841.074902	16.252698	-0.055343	3.781016
282.004295	4833.146742	16.257703	-0.055337	3.778062
281.998958	4825.086847	16.262707	-0.055331	3.775057
282.026434	4817.060667	16.267712	-0.055330	3.772063
282.165157	4809.069204	16.272717	-0.055351	3.769082
281.993701	4801.075340	16.277722	-0.055314	3.766091
282.049526	4793.115745	16.282727	-0.055319	3.763116
282.083613	4785.102061	16.287731	-0.055320	3.760117
281.652865	4777.147498	16.292736	-0.055234	3.757127
281.695743	4769.092003	16.297741	-0.055237	3.754108
281.844836	4761.064684	16.302746	-0.055259	3.751100
281.573922	4753.103056	16.307751	-0.055204	3.748104
281.466426	4745.053872	16.312755	-0.055178	3.745077
281.602198	4737.104757	16.317760	-0.055198	3.742090
281.596876	4729.100300	16.322765	-0.055192	3.739077
281.512393	4721.130474	16.327770	-0.055171	3.736073
281.659744	4713.136764	16.332775	-0.055193	3.733063
281.554881	4705.068618	16.337779	-0.055168	3.730016
281.497637	4697.115663	16.342784	-0.055152	3.727011
281.802322	4689.110625	16.347789	-0.055204	3.723993
281.691111	4681.164886	16.352794	-0.055178	3.720985
281.556164	4673.204062	16.357799	-0.055148	3.717968
281.438899	4665.214033	16.362803	-0.055120	3.714938
281.375475	4657.073205	16.367808	-0.055103	3.711850
281.455269	4649.091944	16.372813	-0.055113	3.708823
281.098851	4641.120770	16.377818	-0.055041	3.705787
281.236934	4633.162758	16.382823	-0.055062	3.702766
281.262310	4625.167669	16.387827	-0.055061	3.699725
281.174050	4617.198868	16.392832	-0.055039	3.696689
281.108928	4609.221221	16.397837	-0.055022	3.693647
281.114143	4601.155541	16.402842	-0.055018	3.690572
280.983447	4593.215112	16.407847	-0.054988	3.687538
280.953969	4585.196161	16.412851	-0.054977	3.684474
281.099358	4577.253932	16.417856	-0.054999	3.681441
280.979087	4569.246957	16.422861	-0.054971	3.678374
280.820352	4561.241135	16.427866	-0.054936	3.675304
280.841330	4553.230057	16.432871	-0.054935	3.672234
280.948542	4545.192230	16.437875	-0.054950	3.669154
280.828616	4537.206469	16.442880	-0.054922	3.666085
280.760638	4529.228822	16.447885	-0.054904	3.663018
280.796584	4521.207852	16.452890	-0.054906	3.659934
280.759732	4513.282086	16.457895	-0.054893	3.656883
280.727540	4505.245171	16.462899	-0.054882	3.653786
280.655251	4497.219445	16.467904	-0.054863	3.650690
280.475453	4489.273434	16.472909	-0.054825	3.647619
280.576766	4481.229250	16.477914	-0.054838	3.644515
280.587351	4473.313582	16.482919	-0.054835	3.641456
280.582228	4465.282224	16.487923	-0.054829	3.638349
280.449824	4457.283472	16.492928	-0.054799	3.635249
280.285197	4449.276933	16.497933	-0.054763	3.632142
280.400119	4441.236948	16.502938	-0.054779	3.629027
280.317498	4433.251373	16.507943	-0.054758	3.625925
280.405512	4425.271979	16.512947	-0.054769	3.622827
280.276101	4417.264074	16.517952	-0.054740	3.619710
280.624089	4409.312127	16.522957	-0.054799	3.616624
280.264608	4401.280539	16.527962	-0.054727	3.613486
280.073215	4393.309041	16.532967	-0.054686	3.610373
280.233593	4385.328348	16.537971	-0.054711	3.607264
280.146118	4377.322560	16.542976	-0.054689	3.604135
280.075280	4369.368890	16.547981	-0.054671	3.601024
280.100759	4361.359401	16.552986	-0.054670	3.597891
280.182123	4353.356061	16.557991	-0.054680	3.594760
280.029834	4345.350191	16.562995	-0.054646	3.591618
280.130495	4337.327590	16.568000	-0.054660	3.588475
280.164450	4329.358934	16.573005	-0.054661	3.585347
280.033985	4321.390080	16.578010	-0.054631	3.582212
279.922793	4313.386395	16.583015	-0.054605	3.579062
279.846204	4305.414248	16.588019	-0.054586	3.575922
279.889891	4297.389659	16.593024	-0.054589	3.572761
279.822292	4289.393763	16.598029	-0.054571	3.569607
279.713110	4281.429378	16.603034	-0.054545	3.566460
279.748635	4273.416385	16.608039	-0.054546	3.563296
279.698409	4265.412096	16.613043	-0.054532	3.560130
279.512331	4257.456561	16.618048	-0.054492	3.556977
279.599892	4249.404336	16.623053	-0.054503	3.553790
279.450344	4241.318698	16.628058	-0.054470	3.550580
279.456772	4233.370371	16.633063	-0.054466	3.547427
279.451821	4225.364746	16.638067	-0.054459	3.544247
279.470982	4217.401403	16.643072	-0.054458	3.541083
279.354565	4209.445960	16.648077	-0.054431	3.537914
279.193898	4201.438345	16.653082	-0.054395	3.534721
279.392427	4193.425769	16.658087	-0.054427	3.531533
279.246822	4185.433907	16.663091	-0.054395	3.528340
279.259421	4177.413884	16.668096	-0.054392	3.525138
279.480022	4169.472757	16.673101	-0.054428	3.521972
279.203804	4161.469740	16.678106	-0.054371	3.518762
279.106160	4153.502574	16.683111	-0.054347	3.515569
279.227751	4145.465909	16.688115	-0.054365	3.512352
279.198216	4137.425623	16.693120	-0.054354	3.509126
279.264865	4129.472386	16.698125	-0.054361	3.505935
279.057078	4121.514195	16.703130	-0.054317	3.502731
279.004342	4113.515677	16.708135	-0.054302	3.499512
279.052821	4105.574041	16.713139	-0.054306	3.496316
278.887008	4097.547153	16.718144	-0.054270	3.493076
279.085105	4089.553528	16.723149	-0.054301	3.489859
278.816280	4081.556598	16.728154	-0.054246	3.486622
278.692838	4073.579752	16.733159	-0.054218	3.483394
278.812957	4065.581936	16.738163	-0.054235	3.480164
278.765697	4057.613181	16.743168	-0.054221	3.476936
278.594496	4049.606204	16.748173	-0.054183	3.473686
278.461167	4041.549947	16.753178	-0.054153	3.470414
278.395763	4033.578203	16.758183	-0.054136	3.467176
278.522877	4025.580176	16.763187	-0.054154	3.463930
278.650488	4017.552728	16.768192	-0.054173	3.460669
278.654641	4009.625455	16.773197	-0.054168	3.457442
278.570740	4001.601614	16.778202	-0.054147	3.454169
278.509896	3993.629470	16.783207	-0.054131	3.450915
278.481658	3985.630148	16.788211	-0.054120	3.447648
278.337622	3977.586697	16.793216	-0.054088	3.444357
278.358637	3969.677241	16.798221	-0.054087	3.441122
278.111495	3961.668190	16.803226	-0.054035	3.437834
278.153251	3953.648735	16.808231	-0.054038	3.434549
278.320739	3945.642655	16.813235	-0.054064	3.431270
278.168502	3937.636864	16.818240	-0.054030	3.427978
278.217413	3929.654239	16.823245	-0.054034	3.424699
278.152867	3921.699184	16.828250	-0.054017	3.421424
277.965632	3913.699749	16.833255	-0.053976	3.418123
278.199274	3905.685500	16.838259	-0.054015	3.414827
278.087843	3897.697606	16.843264	-0.053989	3.411528
277.939731	3889.710717	16.848269	-0.053956	3.408224
277.789811	3881.701604	16.853274	-0.053922	3.404908
277.975164	3873.748594	16.858279	-0.053952	3.401623
278.228029	3865.765906	16.863283	-0.053994	3.398326
278.032635	3857.777198	16.868288	-0.053952	3.395007
277.979996	3849.721263	16.873293	-0.053937	3.391661
277.795659	3841.702409	16.878298	-0.053897	3.388324
277.711935	3833.732594	16.883303	-0.053876	3.385006
277.607837	3825.797844	16.888307	-0.053852	3.381700
277.638233	3817.768150	16.893312	-0.053852	3.378355
277.463547	3809.813934	16.898317	-0.053814	3.375032
277.182024	3801.822164	16.903322	-0.053756	3.371685
277.312221	3793.804110	16.908327	-0.053775	3.368339
277.410265	3785.810887	16.913331	-0.053788	3.364999
277.294030	3777.855835	16.918336	-0.053761	3.361664
277.603358	3769.871464	16.923341	-0.053814	3.358328
277.500258	3761.868636	16.928346	-0.053789	3.354967
277.490264	3753.859167	16.933351	-0.053782	3.351602
277.182919	3745.872313	16.938355	-0.053720	3.348233
277.270934	3737.847541	16.943360	-0.053731	3.344859
277.438719	3729.891311	16.948365	-0.053757	3.341514
277.156183	3721.897053	16.953370	-0.053699	3.338132
277.335773	3713.891439	16.958375	-0.053727	3.334760
277.391898	3705.898725	16.963379	-0.053732	3.331384
277.149709	3697.911442	16.968384	-0.053682	3.327997
277.317518	3689.918535	16.973389	-0.053708	3.324619
276.990615	3681.965413	16.978394	-0.053641	3.321236
276.937181	3673.986886	16.983399	-0.053626	3.317849
277.110985	3665.987642	16.988403	-0.053653	3.314458
276.790761	3657.960246	16.993408	-0.053588	3.311033
276.935958	3649.975533	16.998413	-0.053610	3.307641
276.768561	3641.989392	17.003418	-0.053574	3.304232
276.852971	3633.999378	17.008423	-0.053584	3.300828
277.025839	3626.027944	17.013427	-0.053611	3.297431
276.724014	3618.028273	17.018432	-0.053550	3.294001
276.795226	3610.043740	17.023437	-0.053557	3.290588
276.738421	3602.040350	17.028442	-0.053542	3.287159
276.747435	3594.064164	17.033447	-0.053538	3.283740
276.638937	3586.084352	17.038451	-0.053513	3.280311
276.609857	3578.108659	17.043456	-0.053502	3.276884
276.691633	3570.100076	17.048461	-0.053512	3.273443
276.469535	3562.091246	17.053466	-0.053465	3.269987
276.555949	3554.104901	17.058471	-0.053476	3.266549
276.635300	3546.115274	17.063475	-0.053485	3.263105
276.457189	3538.114237	17.068480	-0.053447	3.259643
276.391065	3530.198143	17.073485	-0.053429	3.256218
276.409611	3522.148529	17.078490	-0.053428	3.252735
276.321834	3514.154047	17.083495	-0.053406	3.249268
276.344524	3506.178104	17.088499	-0.053405	3.245810
276.219676	3498.191227	17.093504	-0.053376	3.242337
276.359860	3490.216428	17.098509	-0.053397	3.238877
276.248320	3482.244760	17.103514	-0.053371	3.235404
276.267489	3474.189319	17.108519	-0.053369	3.231896
276.293092	3466.174221	17.113523	-0.053369	3.228402
276.034772	3458.185010	17.118528	-0.053315	3.224904
275.980772	3450.263311	17.123533	-0.053300	3.221440
275.965244	3442.248122	17.128538	-0.053292	3.217933
275.938585	3434.247002	17.133543	-0.053282	3.214428
275.875732	3426.280097	17.138547	-0.053265	3.210933
275.939358	3418.277267	17.143552	-0.053271	3.207423
276.078278	3410.319371	17.148557	-0.053292	3.203932
275.856984	3402.320496	17.153562	-0.053245	3.200405
275.762606	3394.363148	17.158567	-0.053222	3.196897
275.871088	3386.344327	17.163571	-0.053237	3.193367
275.709759	3378.338825	17.168576	-0.053202	3.189827
275.635366	3370.382723	17.173581	-0.053183	3.186309
275.605893	3362.369773	17.178586	-0.053172	3.182763
275.818525	3354.362287	17.183591	-0.053206	3.179227
275.794361	3346.396919	17.188595	-0.053197	3.175695
275.654753	3338.398105	17.193600	-0.053165	3.172139
275.425005	3330.441608	17.198605	-0.053117	3.168594
275.175167	3322.439249	17.203610	-0.053066	3.165024
275.292560	3314.479152	17.208615	-0.053082	3.161485
275.275944	3306.490523	17.213619	-0.053074	3.157923
275.198329	3298.481892	17.218624	-0.053054	3.154346
275.043499	3290.468262	17.223629	-0.053020	3.150758
275.132692	3282.458850	17.228634	-0.053031	3.147180
275.294887	3274.490386	17.233639	-0.053056	3.143618
275.172371	3266.518412	17.238643	-0.053028	3.140039
275.093281	3258.542290	17.243648	-0.053008	3.136456
275.194395	3250.524959	17.248653	-0.053021	3.132858
274.920764	3242.568995	17.253658	-0.052965	3.129266
274.824009	3234.572271	17.258663	-0.052942	3.125660
274.920846	3226.609261	17.263667	-0.052955	3.122074
274.830270	3218.613806	17.268672	-0.052933	3.118461
274.905447	3210.641575	17.273677	-0.052941	3.114861
274.922092	3202.611256	17.278682	-0.052939	3.111228
274.714616	3194.646416	17.283687	-0.052895	3.107611
274.912897	3186.652469	17.288691	-0.052927	3.103994
274.605294	3178.671671	17.293696	-0.052864	3.100357
274.740400	3170.718441	17.298701	-0.052884	3.096747
274.695136	3162.695885	17.303706	-0.052870	3.093094
274.644247	3154.701202	17.308711	-0.052856	3.089449
274.726483	3146.725805	17.313715	-0.052866	3.085814
274.878909	3138.719196	17.318720	-0.052889	3.082164
274.783799	3130.791421	17.323725	-0.052866	3.078534
274.542754	3122.791763	17.328730	-0.052816	3.074861
274.655371	3114.714097	17.333735	-0.052831	3.071163
274.519644	3106.744150	17.338739	-0.052801	3.067499
274.584456	3098.761971	17.343744	-0.052807	3.063835
274.635986	3090.809661	17.348749	-0.052812	3.060179
274.442543	3082.832313	17.353754	-0.052771	3.056496
274.311475	3074.848808	17.358759	-0.052741	3.052808
274.547895	3066.826414	17.363763	-0.052780	3.049115
274.574923	3058.853419	17.368768	-0.052779	3.045431
274.395915	3050.943687	17.373773	-0.052741	3.041762
274.323182	3042.955168	17.378778	-0.052722	3.038056
274.276933	3034.959568	17.383783	-0.052708	3.034345
274.109835	3026.955423	17.388787	-0.052672	3.030619
273.924587	3018.972490	17.393792	-0.052632	3.026897
274.166746	3010.979734	17.398797	-0.052672	3.023187
274.100847	3002.992015	17.403802	-0.052654	3.019459
273.921732	2995.045418	17.408807	-0.052615	3.015741
273.836854	2987.046107	17.413811	-0.052594	3.011998
273.947130	2979.023634	17.418816	-0.052610	3.008249
273.999704	2971.049803	17.423821	-0.052614	3.004515
273.919853	2963.103799	17.428826	-0.052594	3.000784
274.042085	2955.138424	17.433831	-0.052611	2.997048
273.871321	2947.126328	17.438835	-0.052574	2.993272
273.796970	2939.091033	17.443840	-0.052555	2.989484
274.052800	2931.107021	17.448845	-0.052598	2.985732
273.901680	2923.156350	17.453850	-0.052564	2.981971
273.780016	2915.195491	17.458855	-0.052536	2.978202
273.579255	2907.228165	17.463859	-0.052494	2.974421
273.717778	2899.189383	17.468864	-0.052514	2.970618
273.505866	2891.256868	17.473869	-0.052469	2.966843
273.447002	2883.257728	17.478874	-0.052453	2.963040
273.500360	2875.262077	17.483879	-0.052458	2.959239
273.507678	2867.306520	17.488883	-0.052454	2.955450
273.227770	2859.302523	17.493888	-0.052396	2.951618
273.413564	2851.305788	17.498893	-0.052426	2.947808
273.467689	2843.315277	17.503898	-0.052431	2.943990
273.408671	2835.345419	17.508903	-0.052414	2.940171
273.146328	2827.427558	17.513907	-0.052360	2.936361
273.160908	2819.395741	17.518912	-0.052358	2.932506
273.150200	2811.418126	17.523917	-0.052350	2.928671
272.959627	2803.436904	17.528922	-0.052310	2.924819
272.946659	2795.483766	17.533927	-0.052302	2.920985
272.988186	2787.515064	17.538931	-0.052304	2.917142
272.724522	2779.465742	17.543936	-0.052250	2.913238
272.692429	2771.452819	17.548941	-0.052239	2.909359
272.878910	2763.461935	17.553946	-0.052268	2.905497
272.874514	2755.514861	17.558951	-0.052262	2.901641
272.591381	2747.556510	17.563955	-0.052204	2.897759
272.594723	2739.554160	17.568960	-0.052199	2.893867
272.817495	2731.546559	17.573965	-0.052235	2.889978
272.770571	2723.586626	17.578970	-0.052221	2.886093
272.578031	2715.643428	17.583975	-0.052180	2.882202
272.651705	2707.674355	17.588979	-0.052189	2.878308
272.451976	2699.681594	17.593984	-0.052146	2.874383
272.499812	2691.684242	17.598989	-0.052150	2.870463
272.411377	2683.690831	17.603994	-0.052128	2.866533
272.484631	2675.706769	17.608999	-0.052137	2.862610
272.347831	2667.781313	17.614003	-0.052106	2.858699
272.260512	2659.775793	17.619008	-0.052084	2.854747
272.263088	2651.805378	17.624013	-0.052079	2.850811
272.316465	2643.796693	17.629018	-0.052084	2.846853
272.325335	2635.831877	17.634023	-0.052080	2.842910
272.252227	2627.883005	17.639027	-0.052062	2.838964
271.982517	2619.921703	17.644032	-0.052006	2.834995
271.953536	2611.910415	17.649037	-0.051995	2.831010
271.913866	2603.914149	17.654042	-0.051983	2.827025
271.835701	2595.950466	17.659047	-0.051963	2.823049
271.835647	2587.960370	17.664051	-0.051958	2.819059
271.827815	2579.991835	17.669056	-0.051951	2.815074
271.964541	2571.994946	17.674061	-0.051971	2.811076
271.787294	2564.023687	17.679066	-0.051933	2.807068
271.637487	2556.071931	17.684071	-0.051900	2.803066
272.082921	2548.048670	17.689075	-0.051977	2.799056
271.938433	2540.096785	17.694080	-0.051945	2.795043
271.702520	2532.135442	17.699085	-0.051896	2.791013
271.692427	2524.131749	17.704090	-0.051889	2.786970
271.725197	2516.164917	17.709095	-0.051890	2.782941
271.595157	2508.216842	17.714099	-0.051860	2.778907
271.399667	2500.240660	17.719104	-0.051818	2.774849
271.438287	2492.241559	17.724109	-0.051820	2.770787
271.336934	2484.263788	17.729114	-0.051796	2.766721
271.525037	2476.288387	17.734119	-0.051826	2.762668
271.596005	2468.321208	17.739123	-0.051834	2.758607
271.459127	2460.335819	17.744128	-0.051803	2.754517
271.204963	2452.296936	17.749133	-0.051750	2.750387
271.178807	2444.324329	17.754138	-0.051740	2.746298
271.289514	2436.358386	17.759143	-0.051756	2.742215
271.265581	2428.409246	17.764147	-0.051746	2.738127
271.333233	2420.416309	17.769152	-0.051753	2.734015
271.273820	2412.439545	17.774157	-0.051737	2.729898
270.965434	2404.495376	17.779162	-0.051674	2.725776
270.869749	2396.544712	17.784167	-0.051651	2.721657
271.034037	2388.569717	17.789171	-0.051676	2.717536
271.139537	2380.549410	17.794176	-0.051691	2.713381
271.017363	2372.591974	17.799181	-0.051663	2.709239
270.686986	2364.628564	17.804186	-0.051596	2.705074
270.921009	2356.647578	17.809191	-0.051634	2.700928
270.880095	2348.692037	17.814195	-0.051621	2.696772
270.881730	2340.691153	17.819200	-0.051616	2.692589
270.798867	2332.737313	17.824205	-0.051596	2.688419
270.512677	2324.784134	17.829210	-0.051537	2.684229
270.618437	2316.794338	17.834215	-0.051552	2.680039
270.841747	2308.842459	17.839219	-0.051588	2.675870
270.583272	2300.837581	17.844224	-0.051534	2.671635
270.404675	2292.885482	17.849229	-0.051496	2.667427
270.476262	2284.883708	17.854234	-0.051504	2.663201
270.466622	2276.922759	17.859239	-0.051497	2.658986
270.573642	2268.947249	17.864243	-0.051512	2.654763
270.362016	2260.955505	17.869248	-0.051467	2.650505
270.392426	2252.996914	17.874253	-0.051467	2.646272
270.206208	2245.043659	17.879258	-0.051427	2.642022
270.110000	2237.107735	17.884263	-0.051404	2.637780
270.290079	2229.089642	17.889267	-0.051432	2.633506
270.311940	2221.088525	17.894272	-0.051431	2.629223
270.149289	2213.161309	17.899277	-0.051396	2.624961
270.041719	2205.192921	17.904282	-0.051370	2.620673
270.010040	2197.234033	17.909287	-0.051359	2.616389
269.905719	2189.258140	17.914291	-0.051334	2.612083
269.990799	2181.248522	17.919296	-0.051345	2.607764
270.130071	2173.294985	17.924301	-0.051366	2.603473
270.020345	2165.336555	17.929306	-0.051340	2.599155
269.755174	2157.403628	17.934311	-0.051285	2.594833
269.729122	2149.221428	17.939315	-0.051275	2.590384
269.886714	2141.258352	17.944320	-0.051299	2.586060
269.913995	2133.355159	17.949325	-0.051299	2.581752
269.600018	2125.429185	17.954330	-0.051235	2.577402
269.693976	2117.465464	17.959335	-0.051247	2.573051
269.655162	2109.486632	17.964339	-0.051235	2.568675
269.358290	2101.546303	17.969344	-0.051174	2.564295
269.525102	2093.591183	17.974349	-0.051200	2.559932
269.523386	2085.641688	17.979354	-0.051195	2.555553
269.463021	2077.652484	17.984359	-0.051178	2.551140
269.433778	2069.685881	17.989363	-0.051167	2.546734
269.421803	2061.711166	17.994368	-0.051160	2.542317
269.520803	2053.758956	17.999373	-0.051173	2.537913
269.263718	2045.806109	18.004378	-0.051120	2.533475
269.405915	2037.802905	18.009383	-0.051141	2.529030
269.454991	2029.855237	18.014387	-0.051145	2.524602
269.317118	2021.899639	18.019392	-0.051114	2.520148
269.340905	2013.954445	18.024397	-0.051113	2.515703
269.048767	2005.971497	18.029402	-0.051054	2.511207
269.001155	1997.983777	18.034407	-0.051039	2.506718
269.047191	1990.021607	18.039411	-0.051043	2.502241
268.990739	1982.066954	18.044416	-0.051027	2.497754
268.959706	1974.117816	18.049421	-0.051016	2.493263
268.698360	1966.154926	18.054426	-0.050962	2.488739
268.707881	1958.176234	18.059431	-0.050958	2.484219
268.764337	1950.230958	18.064435	-0.050964	2.479712
268.445901	1942.314004	18.069440	-0.050899	2.475186
268.629188	1934.292473	18.074445	-0.050928	2.470628
268.810286	1926.282629	18.079450	-0.050956	2.466069
268.583277	1918.367226	18.084455	-0.050909	2.461525
268.609277	1910.410891	18.089459	-0.050908	2.456969
268.734584	1902.427759	18.094464	-0.050927	2.452395
268.668468	1894.479662	18.099469	-0.050909	2.447819
268.509573	1886.526983	18.104474	-0.050874	2.443225
268.209967	1878.619484	18.109479	-0.050813	2.438637
268.312748	1870.627653	18.114483	-0.050827	2.434023
268.158003	1862.589615	18.119488	-0.050793	2.429353
268.297213	1854.616382	18.124493	-0.050813	2.424735
268.151870	1846.676597	18.129498	-0.050781	2.420105
268.083859	1838.746123	18.134503	-0.050763	2.415477
267.934780	1830.788493	18.139507	-0.050730	2.410819
267.963374	1822.809656	18.144512	-0.050730	2.406153
268.063013	1814.869536	18.149517	-0.050744	2.401506
267.959280	1806.928009	18.154522	-0.050719	2.396834
267.829763	1798.957769	18.159527	-0.050690	2.392133
267.927925	1790.983149	18.164531	-0.050703	2.387439
267.824281	1783.023443	18.169536	-0.050678	2.382728
267.777202	1775.093028	18.174541	-0.050664	2.378029
267.712160	1767.137340	18.179546	-0.050647	2.373305
267.883408	1759.135059	18.184551	-0.050673	2.368563
267.628298	1751.231488	18.189555	-0.050620	2.363835
267.442970	1743.286391	18.194560	-0.050581	2.359079
267.624894	1735.324793	18.199565	-0.050609	2.354333
267.541560	1727.311138	18.204570	-0.050588	2.349525
267.497897	1719.355314	18.209575	-0.050575	2.344745
267.552944	1711.423342	18.214579	-0.050580	2.339977
267.332418	1703.482051	18.219584	-0.050534	2.335172
267.293105	1695.525888	18.224589	-0.050521	2.330363
267.367102	1687.546520	18.229594	-0.050530	2.325539
267.275249	1679.601382	18.234599	-0.050507	2.320711
267.229168	1671.677604	18.239603	-0.050494	2.315891
267.084269	1663.708595	18.244608	-0.050461	2.311025
267.174295	1655.745486	18.249613	-0.050473	2.306171
267.070144	1647.803520	18.254618	-0.050448	2.301305
267.175880	1639.835599	18.259623	-0.050463	2.296429
267.074894	1631.894922	18.264627	-0.050438	2.291543
267.064969	1623.925770	18.269632	-0.050431	2.286636
267.026399	1616.011791	18.274637	-0.050419	2.281750
266.951548	1608.074389	18.279642	-0.050400	2.276836
267.012986	1600.060570	18.284647	-0.050406	2.271876
266.928206	1592.085702	18.289651	-0.050385	2.266916
266.744648	1584.151051	18.294656	-0.050345	2.261963
266.796269	1576.209985	18.299661	-0.050350	2.257014
266.610060	1568.284435	18.304666	-0.050310	2.252044
266.502558	1560.326708	18.309671	-0.050285	2.247049
266.477545	1552.394106	18.314675	-0.050275	2.242067
266.611445	1544.425978	18.319680	-0.050294	2.237064
266.486727	1536.499364	18.324685	-0.050266	2.232054
266.272335	1528.542000	18.329690	-0.050221	2.227006
266.252646	1520.600375	18.334695	-0.050212	2.221973
266.338239	1512.661469	18.339699	-0.050222	2.216939
266.193555	1504.705764	18.344704	-0.050190	2.211863
266.301679	1496.744059	18.349709	-0.050205	2.206794
266.290115	1488.808895	18.354714	-0.050198	2.201720
266.167705	1480.896472	18.359719	-0.050170	2.196639
266.354131	1472.898813	18.364723	-0.050199	2.191518
266.140982	1464.953251	18.369728	-0.050154	2.186384
266.149769	1457.034414	18.374733	-0.050150	2.181274
265.908301	1449.125520	18.379738	-0.050100	2.176136
265.973052	1441.153222	18.384743	-0.050107	2.170973
266.011502	1433.202851	18.389747	-0.050109	2.165809
265.758103	1425.289774	18.394752	-0.050057	2.160630
265.997266	1417.344404	18.399757	-0.050096	2.155464
265.753303	1409.399999	18.404762	-0.050045	2.150241
265.602602	1401.471692	18.409767	-0.050012	2.145024
265.631645	1393.529426	18.414771	-0.050012	2.139802
265.575704	1385.600732	18.419776	-0.049996	2.134568
265.633782	1377.633853	18.424781	-0.050002	2.129307
265.638960	1369.690918	18.429786	-0.049998	2.124044
265.566262	1361.781917	18.434791	-0.049979	2.118783
265.584060	1353.833659	18.439795	-0.049977	2.113491
265.309331	1345.854592	18.444800	-0.049920	2.108137
265.385051	1337.921922	18.449805	-0.049929	2.102834
265.287823	1330.000545	18.454810	-0.049906	2.097509
265.209864	1322.067808	18.459815	-0.049886	2.092165
265.212560	1314.137658	18.464819	-0.049881	2.086816
265.074132	1306.213523	18.469824	-0.049850	2.081444
265.239773	1298.278539	18.474829	-0.049876	2.076080
265.002634	1290.352907	18.479834	-0.049827	2.070669
265.075462	1282.393298	18.484839	-0.049835	2.065252
265.067293	1274.491202	18.489843	-0.049828	2.059852
264.926040	1266.580596	18.494848	-0.049797	2.054418
265.072742	1258.607503	18.499853	-0.049819	2.048955
264.851488	1250.716997	18.504858	-0.049772	2.043498
264.595052	1242.833246	18.509863	-0.049719	2.038028
264.733935	1234.863605	18.514867	-0.049740	2.032523
264.760005	1226.894772	18.519872	-0.049739	2.026992
264.644522	1218.986657	18.524877	-0.049713	2.021474
264.472641	1211.091785	18.529882	-0.049675	2.015945
264.378655	1203.157289	18.534887	-0.049653	2.010380
264.324867	1195.234860	18.539891	-0.049637	2.004813
264.253299	1187.317385	18.544896	-0.049619	1.999231
264.305305	1179.386261	18.549901	-0.049623	1.993637
264.316612	1171.428773	18.554906	-0.049620	1.988005
264.162411	1163.534681	18.559911	-0.049586	1.982384
264.414281	1155.589422	18.564915	-0.049628	1.976754
264.284196	1147.661565	18.569920	-0.049598	1.971079
264.322045	1139.740665	18.574925	-0.049600	1.965411
264.035018	1131.876835	18.579930	-0.049541	1.959733
264.056641	1123.951027	18.584935	-0.049540	1.954027
264.291282	1115.943008	18.589939	-0.049579	1.948268
263.954519	1108.067495	18.594944	-0.049511	1.942525
264.025435	1100.152711	18.599949	-0.049519	1.936782
264.068525	1092.208831	18.604954	-0.049521	1.930997
264.037777	1084.298329	18.609959	-0.049511	1.925211
263.706146	1076.460844	18.614963	-0.049444	1.919427
263.832250	1068.512133	18.619968	-0.049462	1.913596
263.915367	1060.569510	18.624973	-0.049472	1.907746
263.644157	1052.699988	18.629978	-0.049416	1.901892
263.585396	1044.791371	18.634983	-0.049400	1.896016
263.613851	1036.867246	18.639987	-0.049400	1.890119
263.390387	1028.979186	18.644992	-0.049353	1.884202
263.501237	1021.069726	18.649997	-0.049369	1.878289
263.496004	1013.144682	18.655002	-0.049363	1.872332
263.298486	1005.238838	18.660007	-0.049321	1.866348
263.499241	997.309143	18.665011	-0.049353	1.860373
263.409448	989.419194	18.670016	-0.049331	1.854375
263.265928	981.527427	18.675021	-0.049299	1.848350
263.054137	973.642779	18.680026	-0.049254	1.842303
262.972111	965.764232	18.685031	-0.049234	1.836255
263.078317	957.826778	18.690035	-0.049248	1.830165
262.954801	949.930788	18.695040	-0.049220	1.824059
262.892326	942.050485	18.700045	-0.049203	1.817952
262.780745	934.150282	18.705050	-0.049177	1.811803
262.801605	926.240289	18.710055	-0.049176	1.805641
262.684175	918.372260	18.715059	-0.049149	1.799474
262.535777	910.466952	18.720064	-0.049116	1.793253
262.634480	902.517386	18.725069	-0.049129	1.787006
262.660322	894.621395	18.730074	-0.049128	1.780770
262.696442	886.737637	18.735079	-0.049130	1.774523
262.741789	878.837630	18.740083	-0.049133	1.768242
262.532935	870.974796	18.745088	-0.049089	1.761937
262.468021	863.124784	18.750093	-0.049072	1.755638
262.512204	855.198152	18.755098	-0.049075	1.749268
262.303103	847.345727	18.760103	-0.049031	1.742902
262.380082	839.457509	18.765107	-0.049040	1.736521
262.389399	831.552256	18.770112	-0.049036	1.730093
262.418680	823.683873	18.775117	-0.049037	1.723674
262.059425	815.864737	18.780122	-0.048964	1.717222
262.045167	807.958264	18.785127	-0.048957	1.710718
262.093295	800.064625	18.790131	-0.048960	1.704207
261.742247	792.236030	18.795136	-0.048890	1.697674
261.957744	784.323251	18.800141	-0.048925	1.691119
261.858371	776.453379	18.805146	-0.048901	1.684534
261.854022	768.590169	18.810151	-0.048895	1.677940
261.747221	760.731674	18.815155	-0.048870	1.671311
261.799645	752.830643	18.820160	-0.048874	1.664641
261.672698	745.009324	18.825165	-0.048846	1.657987
261.610350	737.130006	18.830170	-0.048829	1.651266
261.536849	729.278355	18.835175	-0.048810	1.644540
261.622368	721.420230	18.840179	-0.048821	1.637802
261.714792	713.490776	18.845184	-0.048833	1.630976
261.410289	705.665020	18.850189	-0.048771	1.624156
261.367032	697.817667	18.855194	-0.048757	1.617325
261.454845	689.933037	18.860199	-0.048769	1.610450
261.354470	682.102164	18.865203	-0.048745	1.603567
261.162385	674.283617	18.870208	-0.048704	1.596652
261.319152	666.406344	18.875213	-0.048728	1.589704
260.931537	658.613426	18.880218	-0.048650	1.582723
260.795933	650.780578	18.885223	-0.048620	1.575712
260.876385	642.918259	18.890227	-0.048630	1.568674
260.833780	635.071863	18.895232	-0.048617	1.561601
260.771757	627.256725	18.900237	-0.048600	1.554521
260.713031	619.397823	18.905242	-0.048584	1.547369
260.684389	611.559102	18.910247	-0.048573	1.540207
260.566242	603.753667	18.915251	-0.048546	1.533029
260.445407	595.907724	18.920256	-0.048518	1.525779
260.594522	588.083439	18.925261	-0.048541	1.518555
260.435650	580.266648	18.930266	-0.048506	1.511257
260.300323	572.444566	18.935271	-0.048476	1.503923
260.339889	564.631650	18.940275	-0.048478	1.496587
260.203810	556.814708	18.945280	-0.048447	1.489185
260.255731	548.997556	18.950285	-0.048452	1.481774
260.285458	541.181355	18.955290	-0.048452	1.474324
260.185021	533.331027	18.960295	-0.048428	1.466783
260.097435	525.551620	18.965299	-0.048407	1.459273
259.859605	517.771062	18.970304	-0.048358	1.451699
259.883797	509.957134	18.975309	-0.048357	1.444095
259.829715	502.178674	18.980314	-0.048342	1.436473
259.777781	494.370382	18.985319	-0.048327	1.428781
259.713023	486.595508	18.990323	-0.048310	1.421078
259.400514	478.849112	18.995328	-0.048246	1.413321
259.472932	471.036501	19.000333	-0.048255	1.405519
259.469924	463.261609	19.005338	-0.048249	1.397698
259.647294	455.426155	19.010343	-0.048277	1.389802
259.586872	447.662744	19.015347	-0.048260	1.381895
259.234017	439.946112	19.020352	-0.048190	1.373940
259.282006	432.159667	19.025357	-0.048193	1.365935
259.087952	424.431800	19.030362	-0.048152	1.357902
258.979628	416.664036	19.035367	-0.048127	1.349795
259.167098	408.877186	19.040371	-0.048157	1.341670
259.071118	401.138074	19.045376	-0.048134	1.333496
259.007331	393.393022	19.050381	-0.048117	1.325271
258.729464	385.696442	19.055386	-0.048060	1.317009
258.781066	377.820821	19.060391	-0.048064	1.308560
258.547064	370.114275	19.065395	-0.048015	1.300188
258.378029	362.401702	19.070400	-0.047979	1.291767
258.415148	354.674379	19.075405	-0.047981	1.283313
258.533529	346.940859	19.080410	-0.047998	1.274811
258.248076	339.256068	19.085415	-0.047939	1.266230
258.305521	331.552320	19.090419	-0.047945	1.257634
258.197644	323.843882	19.095424	-0.047920	1.248942
258.372518	316.130356	19.100429	-0.047947	1.240238
258.072044	308.478276	19.105434	-0.047886	1.231451
258.003613	300.779917	19.110439	-0.047868	1.222592
258.078822	293.098074	19.115443	-0.047877	1.213716
257.969482	285.418705	19.120448	-0.047852	1.204741
257.967686	277.769145	19.125453	-0.047846	1.195755
257.888647	270.100026	19.130458	-0.047827	1.186662
257.707947	262.479165	19.135463	-0.047788	1.177536
257.666787	254.826027	19.140467	-0.047775	1.168329
257.537313	247.202911	19.145472	-0.047746	1.159066
257.470094	239.555069	19.150477	-0.047728	1.149712
257.531455	231.892691	19.155482	-0.047735	1.140290
257.419738	224.286021	19.160487	-0.047709	1.130821
257.465910	216.666646	19.165491	-0.047712	1.121291
257.443618	209.064429	19.170496	-0.047703	1.111687
257.407201	201.470978	19.175501	-0.047691	1.102006
257.392874	193.891414	19.180506	-0.047684	1.092263
257.256666	186.335621	19.185511	-0.047653	1.082435
257.092845	178.802627	19.190515	-0.047618	1.072541
256.867585	171.255519	19.195520	-0.047571	1.062522
256.883722	163.707231	19.200525	-0.047569	1.052462
256.698926	156.193748	19.205530	-0.047530	1.042305
256.546360	148.685765	19.210535	-0.047496	1.032062
256.542550	141.162687	19.215539	-0.047491	1.021732
256.440005	133.667572	19.220544	-0.047466	1.011312
256.385404	126.187053	19.225549	-0.047451	1.000815
256.404292	118.683277	19.230554	-0.047450	0.990192
256.040655	111.255392	19.235559	-0.047377	0.979467
255.934703	103.813011	19.240563	-0.047353	0.968667
255.958038	96.363535	19.245568	-0.047352	0.957768
255.896578	88.941743	19.250573	-0.047336	0.946763
255.894513	81.533586	19.255578	-0.047330	0.935665
255.761688	74.156686	19.260583	-0.047301	0.924446
255.727627	66.795829	19.265587	-0.047290	0.913141
255.414728	59.699699	19.270592	-0.047227	0.902032