Fri Mar 12 11:43:36 2021


Number of Points = 3624

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.807821	0.027536	0.000000	0.000034	0.720541
0.859258	0.021792	0.005005	0.000025	0.720548
0.849451	0.004715	0.010010	0.000027	0.720511
0.801385	-0.128334	0.015014	0.000036	0.720232
0.910241	-0.150526	0.020019	0.000016	0.720226
0.980184	-0.162658	0.025024	0.000003	0.720227
0.910261	-0.147504	0.030029	0.000016	0.720232
0.955851	-0.160133	0.035034	0.000007	0.720223
0.893270	-0.146208	0.040038	0.000019	0.720228
0.819614	-0.134035	0.045043	0.000033	0.720226
0.771949	-0.124548	0.050048	0.000042	0.720228
0.979215	-0.159352	0.055053	0.000003	0.720232
1.053065	-0.176222	0.060058	-0.000011	0.720225
1.012513	-0.164832	0.065062	-0.000003	0.720233
0.845558	-0.138937	0.070067	0.000028	0.720225
0.867463	-0.141562	0.075072	0.000024	0.720228
0.815675	-0.187093	0.080077	0.000034	0.720120
0.992181	-0.330829	0.085082	0.000001	0.719899
0.889689	-0.307142	0.090086	0.000020	0.719909
0.824054	-0.297268	0.095091	0.000033	0.719905
0.881003	-0.307482	0.100096	0.000022	0.719905
0.844675	-0.299699	0.105101	0.000029	0.719908
0.827992	-0.302028	0.110106	0.000032	0.719897
0.887698	-0.435738	0.115110	0.000021	0.719655
0.823915	-0.449949	0.120115	0.000033	0.719604
0.905593	-0.463419	0.125120	0.000018	0.719606
0.881770	-0.456952	0.130125	0.000022	0.719610
0.684381	-0.424801	0.135130	0.000059	0.719604
0.972851	-0.607355	0.140134	0.000005	0.719346
0.956705	-0.641556	0.145139	0.000009	0.719272
0.943405	-0.638349	0.150144	0.000011	0.719274
0.960419	-0.639710	0.155149	0.000008	0.719277
0.962086	-0.754788	0.160154	0.000008	0.719051
0.921758	-0.786843	0.165158	0.000015	0.718973
0.839737	-0.775273	0.170163	0.000031	0.718967
0.913909	-0.794410	0.175168	0.000017	0.718955
0.905105	-0.945414	0.180173	0.000019	0.718654
0.893021	-0.948158	0.185178	0.000021	0.718644
0.998495	-0.963971	0.190182	0.000001	0.718650
0.926466	-1.060368	0.195187	0.000015	0.718434
0.618894	-1.045304	0.200192	0.000072	0.718356
0.843875	-1.082364	0.205197	0.000030	0.718362
0.621700	-1.146798	0.210202	0.000072	0.718156
0.609063	-1.212615	0.215206	0.000074	0.718022
0.751217	-1.239981	0.220211	0.000048	0.718018
0.894733	-1.364049	0.225216	0.000021	0.717823
0.769297	-1.397976	0.230221	0.000045	0.717711
0.784322	-1.405581	0.235226	0.000042	0.717702
0.750678	-1.544394	0.240230	0.000048	0.717415
0.641748	-1.543101	0.245235	0.000069	0.717379
0.685900	-1.596701	0.250240	0.000061	0.717289
0.711001	-1.701590	0.255245	0.000056	0.717090
0.367981	-1.642811	0.260250	0.000120	0.717085
0.326545	-1.758931	0.265254	0.000128	0.716841
0.553123	-1.841482	0.270259	0.000086	0.716757
0.532210	-1.888185	0.275264	0.000090	0.716657
0.635273	-2.008528	0.280269	0.000071	0.716456
0.507560	-1.994719	0.285274	0.000094	0.716438
0.501147	-2.143052	0.290278	0.000096	0.716142
0.337000	-2.117232	0.295283	0.000126	0.716135
0.083180	-2.170303	0.300288	0.000174	0.715940
0.141273	-2.207350	0.305293	0.000163	0.715887
0.111263	-2.294309	0.310298	0.000169	0.715704
0.212622	-2.389057	0.315302	0.000150	0.715552
-0.031384	-2.403489	0.320307	0.000195	0.715437
-0.437853	-2.434698	0.325312	0.000271	0.715231
-1.562230	-2.231711	0.330317	0.000480	0.715237
-1.894487	-2.333693	0.335322	0.000542	0.714917
-2.651244	-2.199144	0.340326	0.000683	0.714916
-2.976778	-2.143935	0.345331	0.000744	0.714910
-2.910817	-2.300231	0.350336	0.000732	0.714623
-3.389942	-2.219622	0.355341	0.000821	0.714614
-4.034179	-2.109205	0.360346	0.000941	0.714605
-3.696076	-2.261649	0.365350	0.000878	0.714422
-4.524056	-2.185459	0.370355	0.001032	0.714280
-4.530920	-2.184307	0.375360	0.001034	0.714280
-4.478611	-2.191968	0.380365	0.001024	0.714283
-5.114397	-2.197261	0.385370	0.001142	0.714048
-5.529922	-2.158928	0.390374	0.001220	0.713977
-5.343149	-2.193885	0.395379	0.001185	0.713973
-5.404834	-2.185048	0.400384	0.001197	0.713969
-5.296793	-2.274667	0.405389	0.001177	0.713829
-6.512998	-2.147416	0.410394	0.001403	0.713651
-5.931918	-2.245795	0.415398	0.001295	0.713661
-6.440489	-2.160084	0.420403	0.001390	0.713651
-6.610805	-2.126906	0.425408	0.001421	0.713657
-6.358310	-2.282852	0.430413	0.001374	0.713436
-7.373190	-2.139855	0.435418	0.001563	0.713361
-7.198037	-2.167091	0.440422	0.001531	0.713369
-7.189730	-2.171467	0.445427	0.001529	0.713363
-7.264202	-2.159133	0.450432	0.001543	0.713361
-6.943838	-2.331753	0.455437	0.001484	0.713131
-8.282553	-2.147196	0.460442	0.001733	0.713023
-8.164058	-2.163203	0.465446	0.001711	0.713033
-7.797582	-2.230610	0.470451	0.001643	0.713029
-8.279385	-2.145581	0.475456	0.001732	0.713027
-8.228745	-2.183502	0.480461	0.001723	0.712970
-9.159330	-2.147712	0.485466	0.001896	0.712711
-8.957552	-2.179932	0.490470	0.001859	0.712718
-9.375357	-2.106814	0.495475	0.001937	0.712715
-9.330165	-2.116074	0.500480	0.001928	0.712713
-8.871484	-2.195755	0.505485	0.001843	0.712717
-9.269055	-2.129809	0.510490	0.001917	0.712707
-9.380972	-2.238974	0.515494	0.001938	0.712450
-9.973485	-2.164428	0.520499	0.002048	0.712388
-10.194179	-2.124391	0.525504	0.002089	0.712389
-9.765410	-2.198275	0.530509	0.002010	0.712394
-10.018342	-2.156138	0.535514	0.002057	0.712388
-9.945310	-2.166557	0.540518	0.002043	0.712393
-10.020650	-2.220715	0.545523	0.002057	0.712259
-11.130051	-2.106781	0.550528	0.002264	0.712092
-10.308982	-2.251627	0.555533	0.002111	0.712095
-11.109857	-2.110638	0.560538	0.002260	0.712091
-11.143774	-2.102276	0.565542	0.002267	0.712096
-10.708705	-2.182729	0.570547	0.002186	0.712090
-10.931179	-2.142140	0.575552	0.002227	0.712091
-11.418570	-2.191525	0.580557	0.002318	0.711820
-12.046229	-2.111231	0.585562	0.002435	0.711757
-11.907418	-2.129459	0.590566	0.002409	0.711770
-11.840274	-2.143726	0.595571	0.002397	0.711765
-12.011263	-2.113954	0.600576	0.002429	0.711764
-11.813562	-2.147218	0.605581	0.002392	0.711767
-12.007775	-2.117849	0.610586	0.002428	0.711757
-12.141882	-2.180218	0.615590	0.002453	0.711585
-12.752252	-2.135786	0.620595	0.002567	0.711456
-12.632917	-2.157551	0.625600	0.002545	0.711455
-12.649644	-2.150180	0.630605	0.002548	0.711464
-12.796976	-2.129006	0.635610	0.002575	0.711454
-12.564969	-2.164941	0.640614	0.002532	0.711464
-12.816508	-2.124924	0.645619	0.002579	0.711455
-13.086335	-2.191979	0.650624	0.002629	0.711225
-13.506478	-2.157197	0.655629	0.002708	0.711145
-13.702449	-2.126062	0.660634	0.002744	0.711137
-13.512651	-2.158116	0.665638	0.002709	0.711141
-13.476887	-2.164481	0.670643	0.002702	0.711141
-13.710456	-2.123830	0.675648	0.002746	0.711139
-13.695052	-2.121835	0.680653	0.002743	0.711148
-14.241152	-2.124003	0.685658	0.002845	0.710949
-14.490757	-2.114354	0.690662	0.002891	0.710880
-14.395813	-2.133338	0.695667	0.002874	0.710875
-14.438651	-2.126713	0.700672	0.002882	0.710873
-14.183018	-2.169405	0.705677	0.002834	0.710879
-14.185063	-2.175445	0.710682	0.002834	0.710866
-14.368231	-2.136346	0.715686	0.002869	0.710879
-14.977410	-2.200239	0.720691	0.002982	0.710534
-15.447846	-2.116437	0.725696	0.003070	0.710534
-15.494754	-2.105061	0.730701	0.003078	0.710540
-15.277708	-2.148734	0.735706	0.003038	0.710530
-14.978494	-2.199078	0.740710	0.002982	0.710536
-15.350873	-2.131929	0.745715	0.003052	0.710538
-15.298168	-2.158273	0.750720	0.003042	0.710504
-15.577233	-2.248830	0.755725	0.003094	0.710223
-16.061597	-2.165786	0.760730	0.003184	0.710217
-16.478952	-2.087300	0.765734	0.003262	0.710225
-16.221673	-2.135447	0.770739	0.003214	0.710220
-16.208296	-2.138799	0.775744	0.003212	0.710218
-16.112274	-2.152623	0.780749	0.003194	0.710224
-16.267926	-2.155772	0.785754	0.003223	0.710163
-16.725349	-2.205336	0.790758	0.003308	0.709901
-16.688891	-2.213700	0.795763	0.003302	0.709897
-17.430976	-2.083277	0.800768	0.003440	0.709893
-17.000212	-2.155704	0.805773	0.003360	0.709902
-17.198479	-2.124306	0.810778	0.003396	0.709894
-17.240808	-2.114138	0.815782	0.003404	0.709899
-16.960712	-2.196568	0.820787	0.003352	0.709834
-17.724986	-2.177879	0.825792	0.003495	0.709599
-17.712385	-2.178439	0.830797	0.003492	0.709602
-18.148127	-2.104989	0.835802	0.003574	0.709593
-17.649899	-2.190379	0.840806	0.003481	0.709600
-17.685772	-2.185461	0.845811	0.003488	0.709597
-18.342508	-2.070597	0.850816	0.003610	0.709593
-17.980729	-2.186339	0.855821	0.003543	0.709490
-18.786229	-2.156651	0.860826	0.003693	0.709262
-18.789529	-2.151920	0.865830	0.003693	0.709270
-19.104378	-2.096697	0.870835	0.003752	0.709268
-18.915969	-2.133973	0.875840	0.003717	0.709261
-18.593612	-2.187204	0.880845	0.003657	0.709269
-19.153761	-2.090993	0.885850	0.003761	0.709262
-18.909577	-2.143046	0.890854	0.003716	0.709245
-19.343473	-2.210812	0.895859	0.003797	0.708954
-19.773770	-2.133296	0.900864	0.003877	0.708956
-19.729984	-2.138441	0.905869	0.003869	0.708961
-19.741906	-2.138920	0.910874	0.003871	0.708956
-19.864095	-2.116238	0.915878	0.003894	0.708957
-19.935053	-2.105105	0.920883	0.003907	0.708954
-19.711444	-2.146158	0.925888	0.003866	0.708952
-20.005063	-2.235549	0.930893	0.003920	0.708668
-20.867875	-2.098130	0.935898	0.004081	0.708635
-20.683406	-2.128078	0.940902	0.004047	0.708641
-20.281342	-2.199340	0.945907	0.003972	0.708642
-20.826403	-2.103472	0.950912	0.004073	0.708639
-20.531419	-2.154325	0.955917	0.004019	0.708642
-20.512762	-2.160019	0.960922	0.004015	0.708637
-21.118143	-2.192764	0.965926	0.004128	0.708356
-21.474801	-2.130746	0.970931	0.004194	0.708352
-21.604365	-2.109126	0.975936	0.004218	0.708349
-21.034966	-2.206631	0.980941	0.004113	0.708357
-21.651426	-2.102670	0.985946	0.004227	0.708345
-21.765127	-2.079164	0.990950	0.004249	0.708352
-21.195761	-2.188855	0.995955	0.004143	0.708335
-22.225386	-2.167139	1.000960	0.004334	0.708011
-22.265373	-2.154319	1.005965	0.004342	0.708022
-22.694396	-2.084268	1.010970	0.004422	0.708009
-22.066292	-2.192630	1.015974	0.004305	0.708016
-22.137916	-2.180128	1.020979	0.004318	0.708016
-22.562778	-2.105991	1.025984	0.004397	0.708012
-22.250811	-2.169607	1.030989	0.004339	0.707996
-23.542373	-2.087030	1.035994	0.004580	0.707700
-23.260639	-2.134826	1.040998	0.004528	0.707705
-23.334246	-2.122827	1.046003	0.004541	0.707702
-23.633421	-2.071245	1.051008	0.004597	0.707699
-23.352379	-2.117867	1.056013	0.004545	0.707706
-23.365433	-2.118490	1.061018	0.004547	0.707700
-23.253772	-2.135583	1.066022	0.004526	0.707705
-23.467155	-2.159606	1.071027	0.004566	0.707581
-24.455408	-2.084633	1.076032	0.004750	0.707378
-23.531278	-2.246468	1.081037	0.004578	0.707383
-24.343017	-2.104417	1.086042	0.004729	0.707378
-24.470161	-2.081746	1.091046	0.004753	0.707378
-23.867913	-2.189592	1.096051	0.004641	0.707377
-24.369270	-2.102553	1.101056	0.004734	0.707372
-24.320805	-2.175746	1.106061	0.004726	0.707242
-25.259288	-2.090851	1.111066	0.004900	0.707077
-24.682300	-2.190541	1.116070	0.004793	0.707083
-25.017501	-2.130629	1.121075	0.004855	0.707083
-25.326487	-2.078383	1.126080	0.004913	0.707078
-24.929467	-2.144789	1.131085	0.004839	0.707086
-25.228469	-2.095178	1.136090	0.004895	0.707079
-25.237915	-2.158214	1.141094	0.004897	0.706949
-25.898427	-2.135847	1.146099	0.005020	0.706757
-26.065437	-2.108906	1.151104	0.005051	0.706751
-26.195532	-2.081589	1.156109	0.005075	0.706759
-26.267124	-2.073522	1.161114	0.005088	0.706750
-25.730844	-2.166115	1.166118	0.004989	0.706756
-25.988998	-2.119702	1.171123	0.005037	0.706757
-25.919436	-2.158518	1.176128	0.005024	0.706703
-26.192607	-2.235770	1.181133	0.005075	0.706450
-26.714103	-2.147503	1.186138	0.005172	0.706441
-27.249277	-2.049610	1.191142	0.005272	0.706446
-26.769617	-2.135105	1.196147	0.005182	0.706446
-26.848384	-2.123270	1.201152	0.005197	0.706441
-27.046442	-2.082636	1.206157	0.005234	0.706452
-26.926036	-2.131591	1.211162	0.005212	0.706396
-27.348636	-2.189213	1.216166	0.005290	0.706129
-27.584312	-2.147310	1.221171	0.005334	0.706129
-28.027319	-2.070778	1.226176	0.005417	0.706124
-27.454570	-2.168132	1.231181	0.005310	0.706133
-27.601314	-2.146469	1.236186	0.005338	0.706124
-27.751232	-2.117174	1.241190	0.005366	0.706129
-27.364122	-2.238582	1.246195	0.005294	0.706024
-28.406841	-2.135099	1.251200	0.005488	0.705858
-28.345763	-2.142292	1.256205	0.005476	0.705865
-28.277396	-2.158857	1.261210	0.005464	0.705856
-28.235177	-2.163814	1.266214	0.005456	0.705861
-28.303181	-2.151644	1.271219	0.005469	0.705861
-28.756919	-2.071333	1.276224	0.005553	0.705860
-28.820900	-2.209224	1.281229	0.005565	0.705560
-29.491555	-2.108008	1.286234	0.005690	0.705523
-29.694054	-2.069923	1.291238	0.005728	0.705527
-29.256166	-2.149024	1.296243	0.005646	0.705525
-29.511850	-2.105686	1.301248	0.005694	0.705520
-29.459096	-2.108449	1.306253	0.005684	0.705533
-29.523101	-2.103043	1.311258	0.005696	0.705521
-29.494218	-2.222517	1.316262	0.005691	0.705291
-30.440284	-2.092007	1.321267	0.005867	0.705214
-30.495825	-2.085277	1.326272	0.005877	0.705207
-29.808810	-2.204022	1.331277	0.005750	0.705215
-30.343990	-2.113026	1.336282	0.005849	0.705206
-30.367946	-2.105995	1.341286	0.005854	0.705211
-30.275548	-2.122769	1.346291	0.005837	0.705211
-30.895879	-2.146916	1.351296	0.005952	0.704939
-31.449519	-2.070221	1.356301	0.006055	0.704895
-31.495044	-2.066553	1.361306	0.006064	0.704886
-31.036141	-2.147891	1.366310	0.005978	0.704887
-31.343536	-2.092734	1.371315	0.006036	0.704887
-31.410567	-2.083372	1.376320	0.006048	0.704882
-30.915262	-2.169223	1.381325	0.005956	0.704887
-31.125759	-2.200159	1.386330	0.005995	0.704749
-32.399306	-2.053917	1.391334	0.006232	0.704586
-31.908402	-2.139839	1.396339	0.006141	0.704589
-32.168875	-2.096183	1.401344	0.006190	0.704583
-31.915977	-2.137776	1.406349	0.006143	0.704590
-32.203186	-2.089198	1.411354	0.006196	0.704585
-31.867525	-2.147599	1.416358	0.006134	0.704588
-31.794068	-2.244036	1.421363	0.006120	0.704420
-33.291418	-2.060135	1.426368	0.006399	0.704252
-32.660376	-2.168721	1.431373	0.006282	0.704260
-32.828230	-2.139058	1.436378	0.006313	0.704259
-32.975327	-2.112051	1.441382	0.006340	0.704261
-32.734695	-2.155021	1.446387	0.006296	0.704261
-32.898658	-2.128685	1.451392	0.006326	0.704255
-33.126759	-2.201044	1.456397	0.006369	0.704027
-34.113335	-2.062644	1.461402	0.006552	0.703951
-33.846436	-2.107628	1.466406	0.006503	0.703956
-33.454699	-2.176765	1.471411	0.006430	0.703957
-34.146875	-2.057878	1.476416	0.006559	0.703948
-33.795181	-2.115271	1.481421	0.006493	0.703959
-33.573995	-2.159187	1.486426	0.006452	0.703950
-34.008698	-2.198412	1.491430	0.006533	0.703714
-34.606130	-2.129449	1.496435	0.006644	0.703638
-34.647973	-2.125191	1.501440	0.006652	0.703632
-34.135680	-2.210718	1.506445	0.006557	0.703643
-34.686166	-2.116934	1.511450	0.006660	0.703635
-34.608186	-2.131216	1.516454	0.006645	0.703634
-34.297868	-2.206494	1.521459	0.006587	0.703593
-35.582438	-2.103370	1.526464	0.006827	0.703339
-35.480264	-2.117558	1.531469	0.006808	0.703347
-35.385351	-2.137140	1.536474	0.006790	0.703342
-35.578792	-2.101715	1.541478	0.006826	0.703343
-35.482626	-2.116185	1.546483	0.006808	0.703349
-35.445359	-2.128428	1.551488	0.006801	0.703337
-35.021777	-2.247321	1.556493	0.006723	0.703250
-36.256940	-2.149961	1.561498	0.006953	0.703002
-36.409466	-2.120207	1.566502	0.006981	0.703007
-36.261593	-2.145251	1.571507	0.006953	0.703009
-36.670934	-2.076547	1.576512	0.007030	0.703000
-36.452598	-2.109710	1.581517	0.006989	0.703012
-36.210648	-2.156204	1.586522	0.006944	0.703005
-36.381192	-2.167367	1.591526	0.006976	0.702921
-37.298057	-2.115415	1.596531	0.007147	0.702696
-37.161930	-2.142499	1.601536	0.007121	0.702690
-36.935521	-2.178997	1.606541	0.007079	0.702698
-37.100658	-2.153099	1.611546	0.007110	0.702690
-37.335591	-2.110931	1.616550	0.007154	0.702691
-37.098759	-2.150910	1.621555	0.007110	0.702695
-37.455381	-2.144092	1.626560	0.007176	0.702580
-38.241997	-2.106231	1.631565	0.007323	0.702373
-38.058525	-2.142296	1.636570	0.007289	0.702367
-38.147081	-2.124761	1.641574	0.007305	0.702370
-38.205679	-2.111988	1.646579	0.007316	0.702375
-38.273211	-2.103683	1.651584	0.007329	0.702367
-38.100654	-2.129308	1.656589	0.007297	0.702377
-38.197359	-2.123562	1.661594	0.007315	0.702354
-38.967664	-2.123962	1.666598	0.007458	0.702075
-38.784426	-2.155740	1.671603	0.007424	0.702077
-39.164708	-2.091937	1.676608	0.007495	0.702069
-38.881675	-2.137611	1.681613	0.007442	0.702078
-38.867997	-2.144943	1.686618	0.007440	0.702068
-39.123059	-2.098490	1.691622	0.007487	0.702070
-39.157374	-2.098846	1.696627	0.007494	0.702057
-39.617928	-2.173548	1.701632	0.007580	0.701740
-39.365637	-2.214052	1.706637	0.007533	0.701749
-40.096476	-2.086579	1.711642	0.007669	0.701743
-39.938312	-2.114041	1.716646	0.007639	0.701744
-39.640424	-2.163602	1.721651	0.007584	0.701751
-39.909222	-2.120446	1.726656	0.007634	0.701742
-39.620801	-2.223512	1.731661	0.007581	0.701637
-40.750913	-2.121896	1.736666	0.007791	0.701435
-40.502618	-2.164968	1.741670	0.007745	0.701437
-40.638682	-2.137189	1.746675	0.007770	0.701444
-40.979160	-2.082404	1.751680	0.007834	0.701432
-40.500856	-2.163137	1.756685	0.007745	0.701441
-40.727438	-2.126002	1.761690	0.007787	0.701434
-40.923883	-2.152067	1.766694	0.007823	0.701311
-41.318881	-2.173584	1.771699	0.007897	0.701124
-41.355317	-2.169699	1.776704	0.007904	0.701119
-41.577518	-2.124711	1.781709	0.007945	0.701130
-41.565406	-2.130716	1.786714	0.007943	0.701122
-41.499652	-2.141046	1.791718	0.007931	0.701125
-41.652853	-2.112832	1.796723	0.007959	0.701126
-41.908251	-2.149161	1.801728	0.008007	0.700960
-42.164495	-2.142253	1.806733	0.008055	0.700882
-42.151029	-2.147728	1.811738	0.008052	0.700875
-42.378531	-2.109577	1.816742	0.008095	0.700870
-42.105941	-2.155521	1.821747	0.008044	0.700876
-42.053472	-2.166756	1.826752	0.008034	0.700872
-42.018951	-2.216470	1.831757	0.008028	0.700783
-43.275112	-2.114607	1.836762	0.008262	0.700536
-42.981742	-2.167069	1.841766	0.008207	0.700535
-43.239082	-2.120246	1.846771	0.008255	0.700537
-43.252107	-2.118916	1.851776	0.008258	0.700535
-42.890590	-2.180412	1.856781	0.008191	0.700541
-43.078612	-2.149569	1.861786	0.008226	0.700535
-43.402883	-2.194212	1.866790	0.008286	0.700328
-43.861203	-2.164160	1.871795	0.008371	0.700223
-44.083340	-2.126423	1.876800	0.008413	0.700219
-44.063349	-2.126824	1.881805	0.008409	0.700225
-44.173628	-2.108843	1.886810	0.008430	0.700222
-43.925641	-2.155483	1.891814	0.008384	0.700217
-43.710028	-2.189539	1.896819	0.008344	0.700225
-44.503237	-2.192438	1.901824	0.008491	0.699932
-44.896156	-2.137399	1.906829	0.008564	0.699902
-44.868250	-2.144213	1.911834	0.008559	0.699898
-44.924777	-2.135624	1.916838	0.008570	0.699895
-44.944862	-2.128765	1.921843	0.008574	0.699901
-44.874900	-2.145464	1.926848	0.008561	0.699893
-44.608167	-2.200025	1.931853	0.008511	0.699879
-45.692777	-2.145841	1.936858	0.008713	0.699596
-45.860646	-2.115011	1.941862	0.008744	0.699598
-45.839870	-2.115055	1.946867	0.008741	0.699605
-45.951504	-2.099213	1.951872	0.008761	0.699597
-45.428596	-2.189731	1.956877	0.008664	0.699602
-45.754744	-2.132173	1.961882	0.008725	0.699601
-46.021827	-2.086070	1.966886	0.008775	0.699597
-46.004501	-2.238146	1.971891	0.008772	0.699295
-46.667824	-2.134941	1.976896	0.008895	0.699264
-46.876787	-2.092285	1.981901	0.008934	0.699275
-46.803385	-2.109403	1.986906	0.008920	0.699267
-46.737808	-2.121090	1.991910	0.008908	0.699267
-46.603775	-2.144217	1.996915	0.008883	0.699268
-46.818783	-2.162710	2.001920	0.008923	0.699153
-47.605447	-2.119061	2.011917	0.009070	0.698956
-47.447617	-2.147116	2.021914	0.009041	0.698956
-47.385775	-2.157052	2.031910	0.009029	0.698958
-47.509509	-2.133430	2.041907	0.009052	0.698961
-47.651725	-2.109280	2.051904	0.009079	0.698958
-47.528207	-2.131754	2.061901	0.009056	0.698957
-47.589660	-2.119393	2.071898	0.009068	0.698960
-47.417961	-2.149037	2.081894	0.009036	0.698962
-47.364221	-2.158144	2.091891	0.009026	0.698962
-47.565123	-2.123181	2.101888	0.009063	0.698961
-47.267662	-2.117212	2.111885	0.009008	0.699080
-46.529540	-2.155653	2.121882	0.008871	0.699269
-46.705674	-2.124109	2.131878	0.008904	0.699269
-46.534412	-2.154713	2.141875	0.008872	0.699269
-46.702946	-2.124678	2.151872	0.008903	0.699269
-46.482850	-2.163645	2.161869	0.008862	0.699269
-46.584587	-2.072905	2.171866	0.008881	0.699417
-45.795050	-2.123046	2.181862	0.008735	0.699600
-45.823303	-2.119107	2.191859	0.008740	0.699598
-45.858401	-2.113717	2.201856	0.008747	0.699596
-45.777113	-2.101594	2.211853	0.008731	0.699650
-45.194604	-2.084239	2.221850	0.008623	0.699896
-44.882311	-2.141534	2.231846	0.008565	0.699892
-44.979206	-2.124430	2.241843	0.008583	0.699892
-45.007624	-2.065999	2.251840	0.008589	0.700000
-44.066831	-2.128117	2.261837	0.008414	0.700214
-44.031903	-2.133983	2.271834	0.008407	0.700215
-44.066792	-2.126858	2.281830	0.008414	0.700216
-43.679885	-2.102691	2.291827	0.008342	0.700405
-43.405831	-2.088907	2.301824	0.008291	0.700532
-43.264748	-2.113818	2.311821	0.008265	0.700532
-43.467880	-2.061925	2.321818	0.008303	0.700564
-42.218554	-2.131567	2.331814	0.008070	0.700874
-42.337758	-2.111296	2.341811	0.008092	0.700872
-42.305864	-2.116080	2.351808	0.008086	0.700873
-42.396089	-2.059935	2.361805	0.008103	0.700954
-41.647033	-2.113940	2.371802	0.007964	0.701115
-41.528052	-2.133135	2.381798	0.007942	0.701119
-41.829931	-2.068830	2.391795	0.007998	0.701140
-40.969570	-2.077039	2.401792	0.007838	0.701434
-40.838250	-2.100671	2.411789	0.007814	0.701433
-41.004677	-2.070438	2.421786	0.007845	0.701434
-40.327720	-2.065302	2.431782	0.007719	0.701689
-40.093838	-2.079184	2.441779	0.007675	0.701745
-39.889554	-2.116020	2.451776	0.007638	0.701744
-39.631370	-2.088150	2.461773	0.007590	0.701893
-39.130727	-2.089626	2.471770	0.007496	0.702071
-39.025062	-2.106751	2.481766	0.007477	0.702074
-38.946066	-2.121593	2.491763	0.007462	0.702072
-38.313689	-2.102739	2.501760	0.007345	0.702338
-38.287226	-2.094066	2.511757	0.007340	0.702365
-38.158083	-2.115917	2.521754	0.007316	0.702367
-37.816820	-2.104879	2.531750	0.007252	0.702512
-37.270920	-2.115035	2.541747	0.007151	0.702688
-37.292565	-2.110502	2.551744	0.007155	0.702690
-37.582648	-2.060813	2.561741	0.007209	0.702685
-36.646238	-2.072480	2.571738	0.007035	0.702999
-36.438217	-2.106265	2.581734	0.006996	0.703005
-36.585788	-2.081060	2.591731	0.007024	0.703003
-35.873515	-2.110091	2.601728	0.006891	0.703200
-35.495664	-2.109432	2.611725	0.006821	0.703338
-35.515351	-2.105984	2.621722	0.006825	0.703337
-35.664304	-2.078636	2.631718	0.006853	0.703339
-35.000058	-2.050567	2.641715	0.006729	0.703634
-34.613159	-2.120577	2.651712	0.006657	0.703632
-34.602157	-2.123026	2.661709	0.006655	0.703631
-34.341487	-2.096316	2.671706	0.006607	0.703778
-33.763615	-2.113588	2.681702	0.006499	0.703951
-33.949763	-2.079222	2.691699	0.006534	0.703953
-33.712325	-2.121655	2.701696	0.006490	0.703953
-33.153429	-2.070127	2.711693	0.006386	0.704257
-32.703248	-2.150100	2.721690	0.006302	0.704258
-32.984157	-2.098375	2.731686	0.006354	0.704261
-32.626830	-2.088089	2.741683	0.006288	0.704410
-31.848537	-2.137168	2.751680	0.006143	0.704590
-32.104714	-2.091365	2.761677	0.006191	0.704591
-31.926739	-2.124087	2.771674	0.006158	0.704588
-31.435083	-2.079710	2.781670	0.006067	0.704854
-31.333974	-2.080530	2.791667	0.006048	0.704889
-31.128562	-2.118221	2.801664	0.006010	0.704886
-31.002774	-2.058436	2.811661	0.005986	0.705052
-30.131857	-2.135233	2.821658	0.005824	0.705209
-30.388249	-2.088267	2.831654	0.005872	0.705212
-30.226734	-2.118210	2.841651	0.005842	0.705209
-29.607737	-2.073572	2.851648	0.005727	0.705521
-29.481314	-2.094889	2.861645	0.005704	0.705523
-29.353890	-2.117473	2.871642	0.005680	0.705523
-29.072690	-2.082323	2.881638	0.005628	0.705695
-28.433340	-2.110918	2.891635	0.005509	0.705866
-28.403165	-2.116437	2.901632	0.005503	0.705866
-28.626373	-2.078030	2.911629	0.005545	0.705863
-27.659671	-2.125620	2.921626	0.005365	0.706113
-27.860320	-2.082217	2.931622	0.005402	0.706129
-27.479473	-2.149819	2.941619	0.005332	0.706129
-27.566664	-2.065175	2.951616	0.005348	0.706268
-26.614164	-2.146092	2.961613	0.005171	0.706446
-26.813767	-2.111390	2.971610	0.005208	0.706444
-26.782124	-2.115693	2.981606	0.005202	0.706447
-25.951522	-2.120347	2.991603	0.005048	0.706735
-25.981591	-2.107346	3.001600	0.005053	0.706750
-25.869339	-2.127884	3.011597	0.005032	0.706748
-25.683675	-2.093020	3.021594	0.004998	0.706885
-24.957891	-2.125183	3.031590	0.004863	0.707080
-24.863088	-2.140938	3.041587	0.004845	0.707082
-25.087289	-2.102477	3.051584	0.004887	0.707079
-24.417221	-2.090878	3.061581	0.004763	0.707341
-24.250732	-2.102039	3.071578	0.004732	0.707378
-24.219488	-2.107359	3.081574	0.004726	0.707379
-23.884345	-2.085517	3.091571	0.004664	0.707542
-23.606105	-2.055383	3.101568	0.004612	0.707702
-23.554224	-2.065512	3.111565	0.004602	0.707700
-23.216823	-2.083511	3.121562	0.004540	0.707784
-22.560283	-2.083432	3.131558	0.004417	0.708019
-22.486454	-2.096497	3.141555	0.004404	0.708019
-22.788964	-2.042252	3.151552	0.004460	0.708019
-21.944925	-2.036706	3.161549	0.004303	0.708332
-21.669049	-2.073965	3.171546	0.004252	0.708356
-21.535859	-2.097104	3.181542	0.004227	0.708357
-21.224121	-2.092230	3.191539	0.004169	0.708477
-20.712702	-2.101591	3.201536	0.004074	0.708641
-20.829747	-2.079739	3.211533	0.004096	0.708643
-20.651069	-2.111843	3.221530	0.004063	0.708642
-20.001434	-2.091328	3.231526	0.003942	0.708915
-19.803916	-2.104226	3.241523	0.003905	0.708959
-19.888159	-2.090562	3.251520	0.003921	0.708957
-19.669033	-2.082987	3.261517	0.003880	0.709050
-18.939531	-2.105758	3.271514	0.003745	0.709264
-19.203829	-2.057467	3.281510	0.003794	0.709266
-18.843729	-2.119208	3.291507	0.003727	0.709271
-18.592328	-2.025323	3.301504	0.003680	0.709548
-17.998376	-2.106076	3.311501	0.003570	0.709598
-18.087710	-2.090179	3.321498	0.003587	0.709598
-17.915768	-2.067623	3.331494	0.003555	0.709704
-17.229848	-2.091899	3.341491	0.003427	0.709900
-17.239869	-2.091154	3.351488	0.003429	0.709898
-17.266265	-2.087646	3.361485	0.003434	0.709895
-16.624775	-2.051183	3.371482	0.003315	0.710196
-16.253428	-2.102562	3.381478	0.003246	0.710226
-16.178796	-2.116590	3.391475	0.003232	0.710224
-16.331024	-2.031167	3.401472	0.003260	0.710340
-15.130606	-2.147072	3.411469	0.003037	0.710536
-15.244362	-2.125455	3.421466	0.003058	0.710538
-15.075376	-2.152972	3.431462	0.003027	0.710543
-14.851394	-2.104780	3.441459	0.002985	0.710719
-13.998025	-2.177415	3.451456	0.002826	0.710878
-14.489208	-2.089322	3.461453	0.002918	0.710879
-14.357033	-2.113762	3.471450	0.002893	0.710877
-13.936050	-2.100123	3.481446	0.002815	0.711053
-13.779498	-2.081639	3.491443	0.002786	0.711146
-13.487499	-2.134597	3.501440	0.002732	0.711144
-13.462115	-2.108008	3.511437	0.002727	0.711206
-12.881739	-2.084450	3.521434	0.002619	0.711459
-12.461788	-2.157935	3.531430	0.002541	0.711461
-12.513172	-2.147706	3.541427	0.002551	0.711463
-12.094471	-2.123900	3.551424	0.002473	0.711659
-11.821873	-2.118016	3.561421	0.002422	0.711768
-11.691705	-2.141392	3.571418	0.002398	0.711767
-11.538925	-2.167581	3.581414	0.002370	0.711769
-10.946126	-2.108753	3.591411	0.002259	0.712097
-10.810074	-2.131490	3.601408	0.002234	0.712099
-10.894420	-2.117897	3.611405	0.002250	0.712096
-10.841072	-2.058631	3.621402	0.002240	0.712233
-9.772248	-2.168129	3.631398	0.002041	0.712394
-9.986614	-2.129565	3.641395	0.002081	0.712395
-9.780598	-2.167789	3.651392	0.002043	0.712392
-9.274669	-2.114091	3.661389	0.001949	0.712678
-9.097080	-2.126956	3.671386	0.001916	0.712715
-9.003345	-2.142701	3.681382	0.001899	0.712717
-8.945517	-2.095987	3.691379	0.001888	0.712830
-7.981323	-2.166656	3.701376	0.001708	0.713031
-8.118100	-2.142468	3.711373	0.001734	0.713031
-8.212639	-2.127376	3.721370	0.001752	0.713027
-7.410000	-2.143103	3.731366	0.001602	0.713280
-6.967364	-2.175827	3.741363	0.001520	0.713372
-7.008407	-2.170425	3.751360	0.001528	0.713368
-7.206696	-2.136928	3.761357	0.001565	0.713364
-6.335697	-2.160405	3.771354	0.001403	0.713626
-6.319660	-2.146031	3.781350	0.001400	0.713660
-6.310356	-2.148028	3.791347	0.001398	0.713659
-6.150451	-2.137073	3.801344	0.001369	0.713737
-5.583638	-2.118432	3.811341	0.001263	0.713975
-5.147638	-2.195703	3.821338	0.001182	0.713975
-5.526334	-2.127551	3.831334	0.001253	0.713976
-4.556669	-2.184257	3.841331	0.001072	0.714207
-4.213276	-2.206826	3.851328	0.001008	0.714283
-4.463964	-2.163290	3.861325	0.001055	0.714281
-4.381664	-2.176994	3.871322	0.001040	0.714283
-3.844603	-2.117999	3.881318	0.000940	0.714590
-3.474933	-2.170302	3.891315	0.000871	0.714616
-3.297487	-2.202530	3.901312	0.000838	0.714615
-3.601002	-2.105770	3.911309	0.000895	0.714699
-2.465895	-2.199143	3.921306	0.000684	0.714915
-2.704137	-2.156410	3.931302	0.000728	0.714916
-2.518184	-2.189484	3.941299	0.000694	0.714916
-2.402837	-2.087441	3.951296	0.000672	0.715159
-1.909213	-2.136282	3.961293	0.000580	0.715236
-1.854310	-2.144945	3.971290	0.000570	0.715238
-1.684687	-2.112103	3.981286	0.000539	0.715363
-1.588381	-2.033472	3.991283	0.000521	0.715553
-1.424144	-2.062873	4.001280	0.000490	0.715552
-1.147756	-2.036247	4.011277	0.000439	0.715702
-1.175811	-1.936323	4.021274	0.000444	0.715890
-0.938024	-1.978352	4.031270	0.000400	0.715891
-0.962702	-1.872969	4.041267	0.000405	0.716091
-0.885618	-1.862464	4.051264	0.000390	0.716139
-0.845281	-1.787450	4.061261	0.000383	0.716301
-0.937060	-1.692316	4.071258	0.000400	0.716457
-0.659912	-1.659251	4.081254	0.000349	0.716620
-0.704097	-1.578365	4.091251	0.000357	0.716764
-0.778310	-1.453608	4.101248	0.000371	0.716985
-0.647019	-1.420178	4.111245	0.000346	0.717097
-0.560178	-1.287542	4.121242	0.000330	0.717390
-0.321863	-1.264367	4.131238	0.000286	0.717519
-0.412833	-1.151532	4.141235	0.000303	0.717710
-0.312501	-1.026669	4.151232	0.000284	0.717992
-0.295469	-0.929961	4.161229	0.000281	0.718189
-0.170263	-0.847901	4.171226	0.000258	0.718395
0.004561	-0.747569	4.181222	0.000225	0.718654
-0.361452	-0.552964	4.191219	0.000293	0.718910
-0.140011	-0.467536	4.201216	0.000252	0.719156
-0.124993	-0.338127	4.211213	0.000249	0.719416
0.077285	-0.236192	4.221210	0.000212	0.719688
-0.074578	-0.069033	4.231206	0.000240	0.719964
0.000000	0.103422	4.241203	0.000226	0.720330
-0.085611	0.721452	4.246208	0.000242	0.721516
0.110549	1.947998	4.251213	0.000204	0.723991
0.600313	3.722363	4.256218	0.000112	0.727630
0.518794	6.146720	4.261222	0.000126	0.732313
0.830905	9.013320	4.266227	0.000066	0.737952
1.097444	12.357422	4.271232	0.000014	0.744442
1.637072	16.112795	4.276237	-0.000089	0.751745
2.064306	20.299538	4.281242	-0.000171	0.759746
2.529853	24.868618	4.286246	-0.000261	0.768382
2.945388	29.827431	4.291251	-0.000341	0.777617
3.280709	35.136957	4.296256	-0.000407	0.787350
3.681005	40.755074	4.301261	-0.000485	0.797533
4.017646	46.690268	4.306266	-0.000552	0.808125
4.417262	52.889890	4.311270	-0.000630	0.819057
5.031359	59.329597	4.316275	-0.000749	0.830320
5.496647	66.019881	4.321280	-0.000840	0.841809
5.941963	72.930705	4.326285	-0.000927	0.853505
8.370705	79.710816	4.331290	-0.001383	0.865400
10.076636	86.846789	4.336294	-0.001706	0.877502
10.547619	94.379129	4.341299	-0.001798	0.889725
11.304922	102.012137	4.346304	-0.001944	0.902019
11.864511	109.827804	4.351309	-0.002053	0.914377
12.509185	117.745960	4.356314	-0.002179	0.926749
12.699525	125.848931	4.361318	-0.002219	0.939117
14.109811	133.853407	4.366323	-0.002487	0.951495
14.734654	142.083431	4.371328	-0.002609	0.963843
15.411611	150.384164	4.376333	-0.002740	0.976151
16.865367	158.651523	4.381338	-0.003016	0.988451
17.670685	167.072197	4.386342	-0.003172	1.000656
18.271436	175.571557	4.391347	-0.003289	1.012775
18.857646	184.117305	4.396352	-0.003404	1.024810
22.083403	192.253078	4.401357	-0.004009	1.036771
27.863246	200.088320	4.406362	-0.005091	1.048785
28.118508	208.910189	4.411366	-0.005144	1.060701
28.424713	217.736621	4.416371	-0.005207	1.072502
28.730263	226.532193	4.421376	-0.005269	1.084134
29.284955	235.274737	4.426381	-0.005378	1.095629
30.350189	243.927684	4.431386	-0.005582	1.107003
30.991635	252.656580	4.436390	-0.005707	1.118264
31.575382	261.385500	4.441395	-0.005822	1.129400
32.438954	270.061255	4.446400	-0.005988	1.140421
33.296338	278.749259	4.451405	-0.006153	1.151349
33.850669	287.457573	4.456410	-0.006262	1.162136
34.711051	296.082473	4.461414	-0.006428	1.172785
35.353494	304.735279	4.466419	-0.006553	1.183328
36.219420	313.345542	4.471424	-0.006720	1.193771
36.687030	321.985603	4.476429	-0.006812	1.204079
37.678659	330.548980	4.481434	-0.007003	1.214313
38.324983	339.136067	4.486438	-0.007129	1.224421
39.134129	347.719655	4.491443	-0.007285	1.234474
39.892110	356.263830	4.496448	-0.007431	1.244390
40.556863	364.813911	4.501453	-0.007561	1.254217
41.366156	373.325645	4.506458	-0.007717	1.263951
41.953733	381.867149	4.511462	-0.007832	1.273601
42.475323	390.387725	4.516467	-0.007934	1.283144
43.532210	398.821756	4.521472	-0.008137	1.292620
44.141791	407.312384	4.526477	-0.008256	1.302006
44.878288	415.855990	4.531482	-0.008398	1.311404
45.604008	424.339663	4.536486	-0.008539	1.320670
46.507753	432.729669	4.541491	-0.008713	1.329802
47.073749	441.183048	4.546496	-0.008823	1.338879
47.712670	449.590272	4.551501	-0.008948	1.347859
48.230012	458.026909	4.556506	-0.009050	1.356789
48.743635	466.408125	4.561510	-0.009151	1.365602
49.577942	474.764962	4.566515	-0.009311	1.374388
50.174888	483.143710	4.571520	-0.009428	1.383100
51.205621	491.457338	4.576525	-0.009625	1.391764
51.838231	499.831772	4.581530	-0.009749	1.400369
52.397637	508.183774	4.586534	-0.009858	1.408886
52.861748	516.571593	4.591539	-0.009950	1.417372
53.610806	524.879001	4.596544	-0.010095	1.425774
53.995107	533.251866	4.601549	-0.010172	1.434132
54.670796	541.559110	4.606554	-0.010303	1.442424
55.017484	549.898993	4.611558	-0.010373	1.450647
55.688876	558.194318	4.616563	-0.010503	1.458832
56.147845	566.519887	4.621568	-0.010594	1.466967
56.752844	574.856393	4.626573	-0.010712	1.475090
57.929921	583.045356	4.631578	-0.010937	1.483117
58.400562	591.342458	4.636582	-0.011030	1.491094
58.934530	599.633361	4.641587	-0.011134	1.499031
59.253978	607.946188	4.646592	-0.011199	1.506915
59.466881	616.274989	4.651597	-0.011244	1.514756
60.505534	624.451458	4.656602	-0.011443	1.522540
61.058727	632.709078	4.661606	-0.011551	1.530285
61.295734	641.022158	4.666611	-0.011601	1.537996
61.928350	649.237692	4.671616	-0.011724	1.545637
62.574572	657.491828	4.676621	-0.011849	1.553278
62.816691	665.778856	4.681626	-0.011900	1.560851
63.137974	674.022134	4.686630	-0.011965	1.568360
63.684804	682.248991	4.691635	-0.012072	1.575851
64.370243	690.436293	4.696640	-0.012205	1.583291
65.045871	698.636490	4.701645	-0.012336	1.590706
65.407465	706.908315	4.706650	-0.012409	1.598105
66.115422	715.068306	4.711654	-0.012546	1.605420
66.264816	723.364669	4.716659	-0.012579	1.612743
66.844406	731.554168	4.721664	-0.012692	1.619999
67.501945	739.737413	4.726669	-0.012820	1.627229
67.925195	748.030225	4.731674	-0.012904	1.634488
68.338667	756.203287	4.736678	-0.012986	1.641611
68.722364	764.400558	4.741683	-0.013063	1.648719
69.385231	772.575550	4.746688	-0.013192	1.655816
69.870359	780.745533	4.751693	-0.013287	1.662854
70.894234	788.873258	4.756698	-0.013483	1.669899
71.697551	797.040372	4.761702	-0.013638	1.676917
72.129416	805.246489	4.766707	-0.013724	1.683890
72.352861	813.486163	4.771712	-0.013771	1.690834
72.797767	821.680835	4.776717	-0.013859	1.697741
73.484816	829.836604	4.781722	-0.013992	1.704619
73.872994	838.046943	4.786726	-0.014070	1.711476
74.437967	846.215468	4.791731	-0.014180	1.718294
74.910438	854.371496	4.796736	-0.014274	1.725062
75.209840	862.571400	4.801741	-0.014335	1.731817
75.779038	870.726672	4.806746	-0.014446	1.738545
76.348548	878.856369	4.811750	-0.014557	1.745225
76.950426	887.025319	4.816755	-0.014674	1.751915
77.330046	895.214508	4.821760	-0.014750	1.758568
77.831744	903.335894	4.826765	-0.014849	1.765157
78.115753	911.549224	4.831770	-0.014907	1.771768
78.425898	919.718692	4.836774	-0.014970	1.778322
78.801658	927.878527	4.841779	-0.015046	1.784852
79.357180	936.065834	4.846784	-0.015154	1.791403
79.704129	944.234728	4.851789	-0.015224	1.797889
80.210120	952.351569	4.856794	-0.015324	1.804330
80.846881	960.458945	4.861798	-0.015447	1.810757
81.076157	968.630622	4.866803	-0.015495	1.817162
81.391974	976.790486	4.871808	-0.015559	1.823545
81.682673	984.937737	4.876813	-0.015619	1.829893
82.305530	993.054194	4.881818	-0.015740	1.836235
82.652075	1001.185075	4.886822	-0.015810	1.842534
83.002445	1009.334570	4.891827	-0.015880	1.848825
83.787759	1017.428355	4.896832	-0.016032	1.855103
84.096189	1025.569294	4.901837	-0.016094	1.861341
84.421564	1033.742058	4.906842	-0.016160	1.867583
84.933574	1041.892723	4.911846	-0.016261	1.873810
85.323865	1050.008063	4.916851	-0.016339	1.879975
85.766232	1058.127307	4.921856	-0.016426	1.886128
86.389364	1066.230776	4.926861	-0.016548	1.892270
86.979221	1074.340665	4.931866	-0.016663	1.898394
87.264099	1082.477744	4.936870	-0.016721	1.904483
87.617255	1090.628485	4.941875	-0.016792	1.910570
88.140016	1098.757925	4.946880	-0.016895	1.916641
88.506447	1106.865774	4.951885	-0.016968	1.922660
88.829479	1115.004217	4.956890	-0.017034	1.928677
89.536266	1123.093289	4.961894	-0.017170	1.934682
90.077692	1131.196831	4.966899	-0.017276	1.940660
90.572732	1139.315644	4.971904	-0.017374	1.946626
90.675095	1147.517657	4.976909	-0.017398	1.952591
91.470989	1155.595572	4.981914	-0.017552	1.958524
91.698959	1163.706315	4.986918	-0.017599	1.964400
91.949837	1171.834661	4.991923	-0.017651	1.970274
92.663129	1179.915864	4.996928	-0.017789	1.976146
92.720822	1188.047522	5.001933	-0.017805	1.981967
93.137989	1196.156440	5.006938	-0.017888	1.987793
93.364633	1204.311243	5.011942	-0.017936	1.993614
93.817470	1212.391887	5.016947	-0.018025	1.999389
94.652775	1220.420557	5.021952	-0.018186	2.005151
95.179549	1228.514721	5.026957	-0.018289	2.010910
95.725897	1236.641439	5.031962	-0.018396	2.016677
95.843917	1244.775273	5.036966	-0.018423	2.022388
96.140828	1252.899123	5.041971	-0.018484	2.028095
97.079242	1260.989774	5.046976	-0.018664	2.033828
97.289928	1269.090928	5.051981	-0.018708	2.039478
97.836939	1277.164881	5.056986	-0.018815	2.045128
98.255250	1285.278461	5.061990	-0.018899	2.050776
98.788510	1293.375691	5.066995	-0.019003	2.056409
98.923337	1301.518596	5.072000	-0.019033	2.062018
99.090266	1309.634627	5.077005	-0.019070	2.067596
99.744087	1317.712436	5.082010	-0.019197	2.073181
100.101621	1325.798859	5.087014	-0.019268	2.078728
100.593609	1333.868989	5.092019	-0.019365	2.084262
100.927005	1341.982402	5.097024	-0.019433	2.089796
101.465404	1350.055944	5.102029	-0.019538	2.095307
101.884963	1358.162840	5.107034	-0.019621	2.100815
102.260499	1366.259147	5.112038	-0.019697	2.106297
102.513415	1374.409488	5.117043	-0.019749	2.111789
102.908330	1382.528994	5.122048	-0.019828	2.117260
103.278286	1390.576688	5.127053	-0.019902	2.122666
103.757850	1398.652197	5.132058	-0.019996	2.128087
104.217811	1406.739257	5.137062	-0.020087	2.133500
104.648842	1414.813142	5.142067	-0.020173	2.138888
105.002558	1422.899409	5.147072	-0.020244	2.144263
105.369132	1430.975944	5.152077	-0.020317	2.149620
105.886308	1439.085867	5.157082	-0.020419	2.154999
106.339809	1447.130194	5.162086	-0.020508	2.160316
106.745761	1455.202426	5.167091	-0.020589	2.165633
107.095187	1463.311006	5.172096	-0.020659	2.170955
107.513871	1471.400138	5.177101	-0.020743	2.176259
108.006224	1479.478405	5.182106	-0.020840	2.181548
108.417899	1487.558414	5.187110	-0.020921	2.186819
108.784063	1495.677258	5.192115	-0.020995	2.192098
109.177730	1503.780788	5.197120	-0.021073	2.197357
109.423165	1511.854957	5.202125	-0.021124	2.202570
109.750208	1519.936214	5.207130	-0.021190	2.207784
109.972096	1528.035022	5.212134	-0.021237	2.212986
110.347737	1536.110885	5.217139	-0.021312	2.218176
110.832575	1544.171232	5.222144	-0.021408	2.223353
111.095849	1552.260641	5.227149	-0.021462	2.228517
111.616601	1560.342584	5.232154	-0.021564	2.233687
112.159117	1568.377836	5.237158	-0.021670	2.238817
112.489704	1576.438476	5.242163	-0.021737	2.243933
112.895192	1584.530898	5.247168	-0.021818	2.249063
113.121394	1592.641684	5.252173	-0.021865	2.254178
113.762256	1600.690480	5.257178	-0.021990	2.259278
114.184755	1608.741509	5.262182	-0.022073	2.264349
114.490338	1616.840882	5.267187	-0.022136	2.269429
114.848665	1625.022374	5.272192	-0.022208	2.274553
114.803310	1633.094961	5.277197	-0.022204	2.279563
115.474649	1641.111827	5.282202	-0.022335	2.284589
115.614527	1649.192538	5.287206	-0.022366	2.289597
115.758329	1657.293805	5.292211	-0.022398	2.294608
116.183863	1665.345742	5.297216	-0.022482	2.299602
116.410038	1673.398588	5.302221	-0.022530	2.304568
116.942271	1681.448694	5.307226	-0.022634	2.309547
117.450174	1689.518860	5.312230	-0.022734	2.314526
117.709357	1697.570348	5.317235	-0.022787	2.319462
118.225597	1705.622313	5.322240	-0.022888	2.324409
118.511176	1713.697774	5.327245	-0.022947	2.329340
118.874002	1721.799112	5.332250	-0.023020	2.334283
119.359571	1729.828129	5.337254	-0.023115	2.339182
119.714969	1737.899742	5.342259	-0.023187	2.344086
120.362279	1745.964778	5.347264	-0.023312	2.348999
120.753642	1754.067744	5.352269	-0.023390	2.353904
121.130168	1762.132085	5.357274	-0.023466	2.358774
121.306413	1770.198625	5.362278	-0.023504	2.363619
121.567775	1778.269335	5.367283	-0.023558	2.368463
122.029212	1786.355782	5.372288	-0.023649	2.373323
122.252205	1794.438117	5.377293	-0.023696	2.378151
122.721746	1802.476876	5.382298	-0.023788	2.382964
122.917989	1810.559843	5.387302	-0.023830	2.387770
123.377180	1818.629098	5.392307	-0.023921	2.392580
123.631508	1826.707059	5.397312	-0.023973	2.397370
124.053805	1834.733342	5.402317	-0.024057	2.402132
124.534254	1842.784575	5.407322	-0.024152	2.406904
124.684255	1850.886455	5.412326	-0.024185	2.411670
124.786714	1858.971567	5.417331	-0.024209	2.416414
125.365039	1866.988988	5.422336	-0.024322	2.421145
125.697563	1875.031441	5.427341	-0.024389	2.425863
126.018580	1883.146846	5.432346	-0.024454	2.430613
126.455813	1891.250913	5.437350	-0.024541	2.435356
126.807540	1899.270805	5.442355	-0.024611	2.440034
127.042073	1907.319855	5.447360	-0.024660	2.444711
127.350116	1915.358056	5.452365	-0.024723	2.449379
127.975371	1923.410562	5.457370	-0.024844	2.454070
128.221775	1931.480999	5.462374	-0.024896	2.458733
128.509993	1939.521204	5.467379	-0.024954	2.463373
128.919058	1947.577878	5.472384	-0.025036	2.468023
129.033567	1955.674226	5.477389	-0.025062	2.472665
129.528512	1963.715555	5.482394	-0.025160	2.477295
129.944117	1971.741184	5.487398	-0.025242	2.481902
129.997127	1979.837299	5.492403	-0.025257	2.486513
130.287709	1987.920446	5.497408	-0.025317	2.491126
130.558896	1995.972226	5.502413	-0.025372	2.495711
130.704227	2004.046421	5.507418	-0.025405	2.500291
130.968833	2012.084729	5.512422	-0.025459	2.504851
131.295116	2020.144047	5.517427	-0.025525	2.509419
131.934285	2028.218273	5.522432	-0.025649	2.514009
132.342450	2036.228870	5.527437	-0.025730	2.518539
132.606662	2044.286265	5.532442	-0.025785	2.523077
132.986663	2052.315879	5.537446	-0.025861	2.527598
133.324341	2060.394050	5.542451	-0.025929	2.532136
133.824499	2068.465352	5.547456	-0.026027	2.536674
134.478220	2076.453840	5.552461	-0.026154	2.541168
134.920962	2084.503408	5.557466	-0.026242	2.545672
135.089675	2092.618670	5.562470	-0.026278	2.550186
135.242355	2100.699957	5.567475	-0.026312	2.554672
135.686486	2108.738286	5.572480	-0.026400	2.559147
135.714685	2116.793457	5.577485	-0.026410	2.563594
136.142112	2124.858458	5.582490	-0.026495	2.568067
136.521533	2132.907761	5.587494	-0.026571	2.572520
136.826426	2140.947903	5.592499	-0.026633	2.576954
137.001010	2149.036143	5.597504	-0.026671	2.581399
137.158450	2157.082617	5.602509	-0.026705	2.585812
137.623117	2165.136772	5.607514	-0.026797	2.590242
137.955989	2173.375385	5.612518	-0.026864	2.594756
138.155160	2181.344125	5.617523	-0.026906	2.599107
138.462778	2189.357964	5.622528	-0.026969	2.603482
138.626212	2197.360800	5.627533	-0.027005	2.607834
138.927042	2205.424080	5.632538	-0.027066	2.612220
139.377757	2213.456200	5.637542	-0.027155	2.616593
139.470166	2221.504462	5.642547	-0.027177	2.620943
139.695775	2229.550547	5.647552	-0.027224	2.625293
139.871928	2237.594738	5.652557	-0.027262	2.629631
140.231697	2245.659936	5.657562	-0.027335	2.633986
140.580575	2253.674479	5.662566	-0.027405	2.638306
140.797364	2261.714235	5.667571	-0.027450	2.642623
141.371294	2269.741269	5.672576	-0.027562	2.646950
141.230215	2277.840718	5.677581	-0.027541	2.651262
141.636157	2285.898955	5.682586	-0.027622	2.655580
142.076931	2293.915768	5.687590	-0.027709	2.659872
142.221581	2301.963669	5.692595	-0.027741	2.664154
142.456613	2310.041900	5.697600	-0.027790	2.668451
142.644061	2318.111333	5.702605	-0.027831	2.672733
143.002899	2326.147000	5.707610	-0.027903	2.677001
143.487838	2334.161472	5.712614	-0.027998	2.681260
143.721910	2342.184919	5.717619	-0.028047	2.685500
144.150845	2350.223205	5.722624	-0.028132	2.689754
144.544853	2358.278091	5.727629	-0.028210	2.694007
144.700432	2366.350808	5.732634	-0.028245	2.698248
145.441880	2374.346193	5.737638	-0.028388	2.702479
145.781100	2382.384281	5.742643	-0.028456	2.706699
146.196284	2390.463153	5.747648	-0.028539	2.710940
146.245585	2398.518307	5.752653	-0.028553	2.715138
146.447540	2406.589963	5.757658	-0.028596	2.719348
146.590260	2414.627761	5.762662	-0.028628	2.723531
146.818871	2422.673202	5.767667	-0.028675	2.727716
147.252049	2430.745459	5.772672	-0.028761	2.731921
147.308296	2438.803796	5.777677	-0.028777	2.736089
147.783805	2446.829038	5.782682	-0.028871	2.740259
148.020715	2454.857405	5.787686	-0.028920	2.744410
148.449735	2462.882677	5.792691	-0.029005	2.748565
148.759158	2471.017161	5.797696	-0.029068	2.752762
148.929351	2479.080116	5.802701	-0.029105	2.756908
149.374861	2487.079655	5.807706	-0.029193	2.761031
149.616056	2495.089101	5.812710	-0.029243	2.765141
149.459622	2503.155328	5.817715	-0.029219	2.769251
149.945427	2511.192091	5.822720	-0.029315	2.773377
150.337530	2519.207237	5.827725	-0.029393	2.777481
150.624575	2527.245474	5.832730	-0.029452	2.781584
151.049012	2535.277924	5.837734	-0.029536	2.785686
151.459678	2543.296318	5.842739	-0.029617	2.789773
151.677098	2551.395415	5.847744	-0.029663	2.793885
151.856526	2559.416988	5.852749	-0.029702	2.797949
152.208513	2567.452688	5.857754	-0.029772	2.802024
152.457547	2575.501622	5.862758	-0.029824	2.806094
152.552635	2583.555273	5.867763	-0.029847	2.810151
152.662782	2591.640659	5.872768	-0.029873	2.814219
152.903046	2599.657491	5.877773	-0.029923	2.818255
153.284754	2607.689712	5.882778	-0.029999	2.822300
153.681559	2615.727578	5.887782	-0.030078	2.826344
153.918099	2623.771709	5.892787	-0.030127	2.830375
154.292682	2631.848673	5.897792	-0.030202	2.834425
154.617241	2639.827676	5.902797	-0.030268	2.838417
155.143333	2647.843580	5.907802	-0.030371	2.842434
155.410754	2655.901074	5.912806	-0.030426	2.846451
155.391152	2663.964162	5.917811	-0.030427	2.850448
155.778612	2672.022226	5.922816	-0.030505	2.854461
156.110555	2680.032410	5.927821	-0.030572	2.858441
156.395914	2688.092088	5.932826	-0.030630	2.862437
156.556017	2696.144963	5.937830	-0.030665	2.866417
156.767045	2704.157736	5.942835	-0.030710	2.870375
157.116685	2712.253833	5.947840	-0.030780	2.874376
157.150003	2720.294992	5.952845	-0.030791	2.878327
157.933749	2728.260283	5.957850	-0.030942	2.882276
158.413481	2736.276545	5.962854	-0.031037	2.886228
158.376207	2744.355178	5.967859	-0.031035	2.890177
158.783075	2752.437114	5.972864	-0.031116	2.894146
159.105842	2760.456425	5.977869	-0.031181	2.898075
159.554411	2768.472881	5.982874	-0.031270	2.902004
159.794488	2776.543388	5.987878	-0.031320	2.905942
160.028171	2784.572946	5.992883	-0.031369	2.909855
160.384309	2792.713964	5.997888	-0.031440	2.913823
160.448927	2800.734496	6.002893	-0.031457	2.917712
160.734393	2808.748656	6.007898	-0.031516	2.921604
161.127165	2816.756098	6.012902	-0.031594	2.925493
161.506546	2824.738321	6.017907	-0.031670	2.929365
161.853471	2832.805526	6.022912	-0.031740	2.933270
162.189514	2840.834220	6.027917	-0.031807	2.937151
162.520851	2848.856679	6.032922	-0.031874	2.941024
162.809549	2856.890616	6.037926	-0.031933	2.944894
162.971810	2864.936591	6.042931	-0.031969	2.948759
163.400242	2873.002952	6.047936	-0.032054	2.952642
163.508347	2881.065061	6.052941	-0.032079	2.956502
163.573575	2889.083493	6.057946	-0.032096	2.960333
164.048985	2897.077430	6.062950	-0.032190	2.964169
164.278109	2905.111034	6.067955	-0.032238	2.968005
164.621123	2913.180409	6.072960	-0.032307	2.971860
164.831752	2921.217376	6.077965	-0.032351	2.975688
165.081113	2929.258699	6.082970	-0.032403	2.979514
165.265866	2937.300895	6.087974	-0.032443	2.983333
165.665647	2945.330634	6.092979	-0.032522	2.987152
166.042843	2953.394423	6.097984	-0.032598	2.990981
166.031897	2961.462204	6.102989	-0.032601	2.994787
166.110936	2969.471738	6.107994	-0.032621	2.998566
166.495374	2977.483744	6.112998	-0.032697	3.002356
166.826097	2985.501774	6.118003	-0.032764	3.006141
167.188279	2993.532771	6.123008	-0.032837	3.009930
167.244768	3001.592845	6.128013	-0.032853	3.013712
167.672704	3009.602148	6.133018	-0.032937	3.017483
167.960991	3017.656345	6.138022	-0.032996	3.021264
168.275722	3025.643795	6.143027	-0.033060	3.025011
168.850390	3033.684544	6.148032	-0.033172	3.028790
168.919261	3041.758742	6.153037	-0.033190	3.032555
169.292081	3049.804085	6.158042	-0.033265	3.036317
169.766163	3057.814166	6.163046	-0.033358	3.040063
169.961417	3065.831582	6.168051	-0.033400	3.043794
170.264685	3073.894287	6.173056	-0.033462	3.047547
170.479127	3081.938465	6.178061	-0.033507	3.051282
171.123421	3089.963282	6.183066	-0.033632	3.055024
171.292440	3098.009856	6.188070	-0.033668	3.058749
171.468123	3106.046015	6.193075	-0.033706	3.062465
172.029696	3114.085800	6.198080	-0.033816	3.066196
172.016054	3122.133956	6.203085	-0.033819	3.069899
172.367999	3130.249063	6.208090	-0.033890	3.073646
172.771630	3138.252654	6.213094	-0.033970	3.077339
173.198663	3146.205794	6.218099	-0.034054	3.081006
173.543888	3154.204880	6.223104	-0.034124	3.084686
173.656898	3162.276776	6.228109	-0.034150	3.088383
173.991787	3170.298427	6.233114	-0.034218	3.092064
174.235035	3178.357522	6.238118	-0.034268	3.095753
174.267987	3186.383067	6.243123	-0.034280	3.099412
174.741837	3194.403414	6.248128	-0.034373	3.103086
174.976187	3202.433437	6.253133	-0.034422	3.106748
175.249077	3210.474026	6.258138	-0.034478	3.110412
175.773680	3218.507413	6.263142	-0.034581	3.114080
176.031950	3226.537057	6.268147	-0.034634	3.117730
176.309139	3234.588176	6.273152	-0.034691	3.121386
176.437946	3242.577897	6.278157	-0.034720	3.125004
176.637220	3250.648157	6.283162	-0.034762	3.128656
176.672893	3258.708781	6.288166	-0.034774	3.132293
176.997676	3266.732284	6.293171	-0.034840	3.135922
177.253173	3274.760955	6.298176	-0.034892	3.139546
177.531325	3282.761366	6.303181	-0.034949	3.143153
177.716898	3290.824023	6.308186	-0.034989	3.146781
177.977576	3298.869236	6.313190	-0.035043	3.150399
178.249287	3306.906021	6.318195	-0.035099	3.154011
178.452183	3314.951877	6.323200	-0.035142	3.157619
178.662184	3322.970001	6.328205	-0.035186	3.161211
178.771243	3330.958151	6.333210	-0.035211	3.164781
179.349681	3338.999650	6.338214	-0.035324	3.168391
179.509117	3347.022334	6.343219	-0.035359	3.171970
179.764452	3355.093383	6.348224	-0.035412	3.175571
180.187273	3363.063404	6.353229	-0.035496	3.179130
180.359401	3371.120132	6.358234	-0.035533	3.182713
180.378841	3379.173879	6.363238	-0.035542	3.186284
180.770995	3387.170712	6.368243	-0.035620	3.189841
181.240703	3395.229309	6.373248	-0.035713	3.193425
181.408137	3403.249615	6.378253	-0.035749	3.196976
181.786103	3411.273081	6.383258	-0.035825	3.200532
181.923118	3419.298040	6.388262	-0.035855	3.204075
182.240075	3427.326991	6.393267	-0.035920	3.207624
182.538918	3435.400088	6.398272	-0.035980	3.211187
182.943308	3443.407659	6.403277	-0.036061	3.214722
183.133679	3451.454340	6.408282	-0.036101	3.218261
183.316978	3459.511355	6.413286	-0.036141	3.221800
183.714860	3467.462356	6.418291	-0.036220	3.225298
184.223680	3475.513947	6.423296	-0.036320	3.228841
184.233896	3483.624709	6.428301	-0.036327	3.232385
184.463706	3491.668123	6.433306	-0.036375	3.235905
184.927971	3499.634874	6.438310	-0.036467	3.239397
184.919040	3507.665780	6.443315	-0.036470	3.242893
185.234094	3515.688323	6.448320	-0.036534	3.246396
185.607027	3523.679127	6.453325	-0.036609	3.249883
185.852217	3531.759551	6.458330	-0.036660	3.253401
185.943978	3539.794504	6.463334	-0.036682	3.256888
186.260330	3547.782912	6.468339	-0.036746	3.260361
186.953160	3555.772987	6.473344	-0.036880	3.263845
187.361904	3563.794269	6.478349	-0.036961	3.267328
187.731789	3571.869821	6.483354	-0.037035	3.270829
188.085586	3579.938292	6.488358	-0.037106	3.274323
188.039020	3587.977195	6.493363	-0.037103	3.277784
188.353930	3596.003473	6.498368	-0.037167	3.281250
188.524188	3603.976622	6.503373	-0.037204	3.284685
188.912393	3612.020029	6.508378	-0.037281	3.288154
189.173005	3620.080687	6.513382	-0.037335	3.291622
189.639028	3628.091456	6.518387	-0.037427	3.295072
189.942193	3636.127627	6.523392	-0.037488	3.298524
190.127375	3644.155883	6.528397	-0.037528	3.301964
190.318803	3652.177426	6.533402	-0.037569	3.305398
190.632381	3660.243392	6.538406	-0.037633	3.308852
190.814665	3668.298822	6.543411	-0.037672	3.312293
191.066166	3676.338988	6.548416	-0.037724	3.315726
191.396177	3684.305780	6.553421	-0.037790	3.319127
191.500582	3692.321383	6.558426	-0.037815	3.322538
191.582480	3700.348730	6.563430	-0.037835	3.325948
191.961868	3708.325103	6.568435	-0.037911	3.329345
192.294874	3716.413411	6.573440	-0.037978	3.332784
192.368996	3724.473080	6.578445	-0.037997	3.336198
192.753528	3732.424579	6.583450	-0.038074	3.339573
193.210145	3740.450523	6.588454	-0.038164	3.342980
193.272712	3748.518345	6.593459	-0.038181	3.346386
193.423988	3756.570436	6.598464	-0.038215	3.349785
193.654465	3764.618006	6.603469	-0.038263	3.353182
194.034728	3772.643858	6.608474	-0.038339	3.356572
194.038605	3780.653150	6.613478	-0.038345	3.359937
194.198872	3788.681614	6.618483	-0.038380	3.363313
194.531180	3796.718392	6.623488	-0.038447	3.366695
194.978234	3804.711111	6.628493	-0.038535	3.370059
195.064825	3812.778591	6.633498	-0.038556	3.373438
195.380537	3820.822767	6.638502	-0.038620	3.376813
195.797360	3828.803744	6.643507	-0.038703	3.380161
196.144089	3836.844439	6.648512	-0.038773	3.383528
196.225897	3844.886466	6.653517	-0.038793	3.386883
196.345358	3852.915336	6.658522	-0.038821	3.390230
196.743981	3861.039865	6.663526	-0.038900	3.393624
197.009404	3869.035823	6.668531	-0.038955	3.396956
197.457596	3876.995127	6.673536	-0.039043	3.400276
197.709394	3884.995393	6.678541	-0.039095	3.403603
197.991085	3893.010168	6.683546	-0.039153	3.406933
198.366702	3901.034930	6.688550	-0.039228	3.410268
198.542520	3909.092603	6.693555	-0.039266	3.413606
198.691043	3917.134048	6.698560	-0.039299	3.416933
199.096451	3925.109232	6.703565	-0.039380	3.420238
199.333082	3933.138797	6.708570	-0.039429	3.423557
199.644719	3941.194378	6.713574	-0.039492	3.426886
199.872030	3949.207165	6.718579	-0.039540	3.430191
200.292382	3957.246207	6.723584	-0.039623	3.433510
200.371506	3965.298999	6.728589	-0.039643	3.436819
200.625310	3973.287533	6.733594	-0.039695	3.440106
200.908571	3981.302776	6.738598	-0.039753	3.443401
201.212949	3989.347771	6.743603	-0.039815	3.446705
201.290462	3997.400635	6.748608	-0.039835	3.450002
201.462549	4005.465089	6.753613	-0.039872	3.453304
201.711883	4013.469181	6.758618	-0.039924	3.456581
202.068622	4021.486927	6.763622	-0.039995	3.459863
202.048608	4029.495842	6.768627	-0.039997	3.463127
202.278014	4037.549944	6.773632	-0.040045	3.466414
202.520992	4045.536242	6.778637	-0.040095	3.469670
202.890458	4053.619268	6.783642	-0.040169	3.472967
203.142026	4061.666408	6.788646	-0.040221	3.476242
203.036252	4069.633986	6.793651	-0.040206	3.479471
203.425042	4077.660125	6.798656	-0.040284	3.482736
203.589487	4085.666101	6.803661	-0.040320	3.485982
203.939423	4093.658900	6.808666	-0.040390	3.489226
204.235147	4101.721517	6.813670	-0.040450	3.492494
204.395592	4109.755191	6.818675	-0.040485	3.495742
204.841874	4117.762556	6.823680	-0.040574	3.498986
205.167482	4125.763679	6.828685	-0.040640	3.502220
205.272462	4133.783236	6.833690	-0.040664	3.505452
205.392010	4141.828536	6.838694	-0.040692	3.508692
205.715764	4149.861715	6.843699	-0.040757	3.511930
206.018912	4157.925053	6.848704	-0.040819	3.515177
206.205171	4165.926303	6.853709	-0.040859	3.518392
206.262238	4173.978359	6.858714	-0.040874	3.521620
206.554331	4181.977783	6.863718	-0.040934	3.524832
206.770570	4189.995099	6.868723	-0.040979	3.528045
206.941419	4198.046723	6.873728	-0.041016	3.531268
207.164564	4206.070537	6.878733	-0.041063	3.534479
207.413434	4214.099032	6.883738	-0.041115	3.537689
207.688664	4222.140792	6.888742	-0.041171	3.540902
207.872946	4230.108177	6.893747	-0.041211	3.544080
208.238591	4238.186208	6.898752	-0.041284	3.547304
208.588717	4246.210839	6.903757	-0.041354	3.550504
208.860952	4254.326553	6.908762	-0.041410	3.553734
209.240334	4262.345770	6.913766	-0.041486	3.556927
209.099042	4270.273850	6.918771	-0.041465	3.560065
209.556787	4278.273423	6.923776	-0.041555	3.563247
209.775446	4286.321673	6.928781	-0.041601	3.566437
209.872641	4294.323749	6.933786	-0.041624	3.569603
210.037597	4302.400768	6.938790	-0.041660	3.572798
210.372106	4310.403830	6.943795	-0.041728	3.575966
210.614137	4318.387619	6.948800	-0.041778	3.579120
210.693245	4326.426105	6.953805	-0.041798	3.582289
210.890739	4334.406017	6.958810	-0.041840	3.585435
211.272113	4342.466312	6.963814	-0.041916	3.588615
211.393588	4350.522483	6.968819	-0.041944	3.591783
211.789025	4358.531891	6.973824	-0.042023	3.594938
212.049996	4366.542243	6.978829	-0.042076	3.598086
212.190244	4374.560406	6.983834	-0.042108	3.601232
212.637196	4382.544604	6.988838	-0.042196	3.604370
212.720338	4390.594614	6.993843	-0.042217	3.607520
212.985772	4398.632368	6.998848	-0.042271	3.610669
213.109058	4406.664930	7.003853	-0.042300	3.613808
213.254613	4414.690155	7.008858	-0.042332	3.616943
213.648663	4422.717738	7.013862	-0.042410	3.620082
213.789028	4430.728581	7.018867	-0.042442	3.623205
214.242169	4438.759825	7.023872	-0.042531	3.626342
214.408303	4446.770068	7.028877	-0.042567	3.629461
214.556122	4454.836808	7.033882	-0.042600	3.632597
214.710740	4462.892416	7.038886	-0.042634	3.635728
214.912636	4470.883293	7.043891	-0.042677	3.638831
215.147038	4478.902227	7.048896	-0.042726	3.641944
215.492841	4486.874465	7.053901	-0.042795	3.645039
215.416581	4494.957733	7.058906	-0.042786	3.648163
215.729644	4502.991337	7.063910	-0.042850	3.651275
215.857786	4511.006542	7.068915	-0.042879	3.654373
216.081552	4519.014005	7.073920	-0.042926	3.657467
216.416993	4527.031312	7.078925	-0.042993	3.660566
216.529150	4535.032559	7.083930	-0.043019	3.663650
216.500475	4543.120738	7.088934	-0.043019	3.666761
216.661789	4551.111995	7.093939	-0.043054	3.669837
216.883209	4559.157232	7.098944	-0.043101	3.672933
217.045212	4567.206013	7.103949	-0.043136	3.676025
217.307625	4575.163724	7.108954	-0.043190	3.679083
217.641906	4583.186986	7.113958	-0.043258	3.682166
217.708610	4591.191630	7.118963	-0.043275	3.685232
217.902426	4599.230501	7.123968	-0.043316	3.688311
218.089194	4607.292177	7.128973	-0.043356	3.691397
218.124205	4615.298683	7.133978	-0.043368	3.694455
218.285936	4623.350203	7.138982	-0.043403	3.697530
218.626313	4631.312438	7.143987	-0.043472	3.700574
219.025220	4639.333333	7.148992	-0.043551	3.703639
219.277450	4647.374689	7.153997	-0.043604	3.706705
219.526359	4655.384433	7.159002	-0.043655	3.709757
219.990817	4663.509462	7.164006	-0.043747	3.712855
219.996086	4671.555040	7.169011	-0.043753	3.715910
220.238470	4679.520389	7.174016	-0.043803	3.718937
220.602088	4687.548867	7.179021	-0.043876	3.721988
220.708956	4695.459436	7.184026	-0.043901	3.724986
220.856300	4703.549684	7.189030	-0.043934	3.728051
221.121677	4711.547475	7.194035	-0.043988	3.731081
221.359674	4719.575945	7.199040	-0.044038	3.734119
221.414181	4727.618491	7.204045	-0.044053	3.737156
221.661948	4735.602465	7.209050	-0.044105	3.740173
222.147059	4743.620411	7.214054	-0.044200	3.743205
222.374821	4751.631281	7.219059	-0.044248	3.746227
222.264587	4759.705460	7.224064	-0.044232	3.749262
222.576329	4767.735035	7.229069	-0.044296	3.752287
223.018225	4775.741565	7.234074	-0.044383	3.755305
223.218018	4783.779647	7.239078	-0.044425	3.758326
223.223727	4791.789576	7.244083	-0.044432	3.761330
223.431591	4799.804369	7.249088	-0.044475	3.764337
223.758259	4807.843445	7.254093	-0.044541	3.767354
223.709192	4815.836841	7.259098	-0.044537	3.770343
224.109196	4823.911263	7.264102	-0.044617	3.773370
224.083933	4831.922735	7.269107	-0.044618	3.776362
224.457620	4839.896420	7.274112	-0.044692	3.779346
224.532479	4847.984993	7.279117	-0.044712	3.782364
224.813255	4855.947022	7.284122	-0.044769	3.785336
224.884724	4864.031124	7.289126	-0.044787	3.788348
225.229341	4872.024001	7.294131	-0.044857	3.791329
225.351217	4880.085272	7.299136	-0.044885	3.794328
225.657224	4888.091640	7.304141	-0.044947	3.797308
226.075092	4896.047351	7.309146	-0.045030	3.800269
226.259564	4904.076226	7.314150	-0.045069	3.803251
226.434553	4912.090126	7.319155	-0.045107	3.806224
226.580010	4920.120533	7.324160	-0.045139	3.809200
226.814799	4928.167295	7.329165	-0.045188	3.812182
226.965388	4936.183944	7.334170	-0.045222	3.815148
227.317523	4944.207104	7.339174	-0.045292	3.818119
227.358407	4952.212274	7.344179	-0.045305	3.821074
227.524662	4960.221556	7.349184	-0.045341	3.824032
227.848551	4968.298455	7.354189	-0.045407	3.827015
227.978280	4976.271567	7.359194	-0.045436	3.829953
228.126988	4984.338922	7.364198	-0.045469	3.832924
228.228153	4992.329492	7.369203	-0.045493	3.835864
228.397691	5000.313886	7.374208	-0.045530	3.838800
228.520415	5008.394743	7.379213	-0.045558	3.841769
228.908638	5016.317176	7.384218	-0.045635	3.844683
229.150267	5024.438044	7.389222	-0.045685	3.847664
229.213499	5032.413202	7.394227	-0.045702	3.850586
229.526754	5040.466801	7.399232	-0.045766	3.853539
229.892828	5048.519534	7.404237	-0.045839	3.856491
229.794417	5056.479355	7.409242	-0.045826	3.859398
230.056183	5064.535748	7.414246	-0.045880	3.862344
230.332552	5072.529126	7.419251	-0.045936	3.865266
230.448277	5080.588829	7.424256	-0.045963	3.868206
230.701717	5088.643822	7.429261	-0.046016	3.871145
230.824529	5096.879440	7.434266	-0.046044	3.874145
231.303184	5104.840424	7.439270	-0.046138	3.877050
231.281854	5112.723552	7.444275	-0.046139	3.879914
231.667934	5120.734349	7.449280	-0.046216	3.882831
231.849848	5128.715739	7.454285	-0.046255	3.885730
231.787235	5136.694619	7.459290	-0.046249	3.888622
231.982152	5144.770964	7.464294	-0.046290	3.891552
232.240940	5152.794914	7.469299	-0.046344	3.894462
232.414455	5160.795790	7.474304	-0.046381	3.897360
232.586287	5168.813158	7.479309	-0.046418	3.900262
232.760292	5176.831276	7.484314	-0.046456	3.903161
233.280680	5184.882453	7.489318	-0.046558	3.906077
233.367835	5192.848847	7.494323	-0.046579	3.908953
233.580887	5200.908249	7.499328	-0.046624	3.911861
233.737719	5208.937610	7.504333	-0.046659	3.914756
233.779537	5216.930271	7.509338	-0.046672	3.917633
234.099985	5224.919854	7.514342	-0.046736	3.920512
234.437585	5232.911975	7.519347	-0.046804	3.923391
234.522089	5240.962046	7.524352	-0.046825	3.926283
234.750309	5248.991712	7.529357	-0.046873	3.929168
235.000152	5256.996685	7.534362	-0.046925	3.932043
235.171960	5265.035936	7.539366	-0.046962	3.934926
235.145824	5273.050013	7.544371	-0.046962	3.937795
235.313380	5281.054220	7.549376	-0.046999	3.940662
235.774318	5289.076932	7.554381	-0.047090	3.943538
235.838833	5297.074492	7.559386	-0.047107	3.946396
235.946034	5305.137035	7.564390	-0.047132	3.949276
236.377037	5313.172210	7.569395	-0.047217	3.952150
236.627660	5321.216055	7.574400	-0.047269	3.955022
236.780211	5329.225890	7.579405	-0.047303	3.957877
237.068969	5337.190266	7.584410	-0.047362	3.960717
237.503035	5345.218491	7.589414	-0.047448	3.963580
237.475507	5353.233478	7.594419	-0.047448	3.966428
237.733999	5361.266985	7.599424	-0.047501	3.969286
237.984543	5369.311175	7.604429	-0.047553	3.972145
238.081228	5377.316582	7.609434	-0.047576	3.974986
238.232293	5385.339307	7.614438	-0.047609	3.977831
238.532865	5393.326452	7.619443	-0.047671	3.980665
238.532219	5401.355534	7.624448	-0.047676	3.983506
238.683210	5409.377130	7.629453	-0.047709	3.986345
238.990424	5417.390220	7.634458	-0.047771	3.989182
239.255587	5425.464154	7.639462	-0.047826	3.992037
239.180233	5433.505614	7.644467	-0.047817	3.994874
239.702844	5441.482946	7.649472	-0.047919	3.997695
239.933506	5449.496256	7.654477	-0.047968	4.000522
240.147589	5457.470854	7.659482	-0.048013	4.003334
240.323121	5465.569167	7.664486	-0.048050	4.006186
240.426240	5473.569996	7.669491	-0.048075	4.009001
240.696217	5481.601041	7.674496	-0.048130	4.011827
240.800237	5489.666601	7.679501	-0.048155	4.014660
240.893237	5497.661848	7.684506	-0.048177	4.017467
241.245944	5505.656624	7.689510	-0.048248	4.020276
241.376094	5513.651763	7.694515	-0.048278	4.023079
241.408699	5521.694269	7.699520	-0.048289	4.025895
241.713035	5529.706501	7.704525	-0.048351	4.028703
241.754505	5537.731380	7.709530	-0.048364	4.031510
242.077061	5545.882048	7.714534	-0.048429	4.034362
242.431115	5553.851216	7.719539	-0.048500	4.037150
242.569599	5561.793187	7.724544	-0.048531	4.039923
242.722968	5569.816187	7.729549	-0.048565	4.042722
242.876178	5577.787457	7.734554	-0.048598	4.045502
243.423346	5585.844551	7.739558	-0.048705	4.048315
243.406254	5593.849476	7.744563	-0.048707	4.051100
243.557498	5601.895995	7.749568	-0.048741	4.053900
243.926446	5609.943593	7.754573	-0.048815	4.056701
244.066082	5617.870576	7.759578	-0.048846	4.059455
244.276646	5625.945008	7.764582	-0.048890	4.062260
244.405009	5633.919493	7.769587	-0.048919	4.065026
244.786239	5641.945943	7.774592	-0.048995	4.067813
244.872509	5649.962976	7.779597	-0.049017	4.070590
244.868127	5658.011755	7.784602	-0.049021	4.073375
245.192410	5666.080835	7.789606	-0.049087	4.076169
245.553663	5674.014017	7.794611	-0.049159	4.078915
245.839937	5682.044326	7.799616	-0.049217	4.081692
245.968064	5690.041241	7.804621	-0.049246	4.084453
246.043913	5698.086445	7.809626	-0.049266	4.087228
246.186807	5706.078333	7.814630	-0.049298	4.089984
246.474153	5714.124457	7.819635	-0.049356	4.092759
246.583413	5722.174916	7.824640	-0.049382	4.095530
246.779535	5730.191197	7.829645	-0.049424	4.098289
246.779456	5738.163258	7.834650	-0.049429	4.101029
247.232045	5746.198822	7.839654	-0.049518	4.103795
247.283094	5754.218882	7.844659	-0.049533	4.106547
247.449274	5762.241815	7.849664	-0.049569	4.109301
247.709406	5770.345946	7.854669	-0.049623	4.112082
247.894903	5778.328988	7.859674	-0.049662	4.114818
248.047933	5786.381601	7.864678	-0.049696	4.117576
248.069542	5794.332244	7.869683	-0.049705	4.120296
248.206355	5802.355176	7.874688	-0.049736	4.123040
248.371296	5810.357797	7.879693	-0.049772	4.125775
248.553263	5818.361524	7.884698	-0.049811	4.128510
248.884221	5826.424740	7.889702	-0.049878	4.131264
249.065287	5834.468662	7.894707	-0.049916	4.134008
249.037581	5842.489755	7.899712	-0.049916	4.136740
249.256753	5850.462376	7.904717	-0.049962	4.139457
249.396855	5858.473434	7.909722	-0.049994	4.142184
249.861528	5866.529812	7.914726	-0.050085	4.144929
249.900658	5874.571750	7.919731	-0.050098	4.147661
250.221174	5882.542036	7.924736	-0.050163	4.150371
250.425624	5890.619270	7.929741	-0.050206	4.153114
250.399326	5898.627013	7.934746	-0.050206	4.155829
250.747811	5906.607758	7.939750	-0.050276	4.158538
250.878914	5914.607738	7.944755	-0.050306	4.161248
251.207229	5922.602605	7.949760	-0.050372	4.163957
251.244041	5930.670846	7.954765	-0.050384	4.166686
251.496208	5938.625353	7.959770	-0.050436	4.169377
251.803254	5946.709035	7.964774	-0.050499	4.172111
251.893672	5954.753526	7.969779	-0.050521	4.174827
252.204893	5962.759905	7.974784	-0.050584	4.177531
252.418510	5970.755351	7.979789	-0.050629	4.180229
252.606408	5978.741134	7.984794	-0.050669	4.182921
252.917577	5986.807007	7.989798	-0.050732	4.185639
252.978660	5994.834329	7.994803	-0.050749	4.188341
253.005421	6002.832665	7.999808	-0.050759	4.191030
253.152328	6010.950383	8.004813	-0.050791	4.193759
253.260567	6018.940740	8.009818	-0.050817	4.196443
253.533007	6026.896666	8.014822	-0.050873	4.199115
253.554094	6034.899158	8.019827	-0.050882	4.201799
253.969471	6042.847945	8.024832	-0.050964	4.204467
254.272100	6050.935991	8.029837	-0.051026	4.207179
254.328435	6058.905364	8.034842	-0.051041	4.209846
254.481160	6066.970259	8.039846	-0.051075	4.212545
254.593523	6074.994902	8.044851	-0.051101	4.215229
254.837054	6082.961866	8.049856	-0.051152	4.217892
255.430531	6090.999297	8.054861	-0.051267	4.220581
255.727583	6098.974138	8.059866	-0.051328	4.223245
256.120061	6107.013154	8.064870	-0.051406	4.225929
256.293703	6115.015115	8.069875	-0.051444	4.228597
256.513568	6123.066821	8.074880	-0.051490	4.231280
256.870062	6131.184549	8.079885	-0.051561	4.233984
256.910864	6139.153268	8.084890	-0.051574	4.236634
257.028043	6147.156774	8.089894	-0.051601	4.239295
257.106777	6155.186200	8.094899	-0.051621	4.241963
257.358722	6163.136811	8.099904	-0.051673	4.244604
257.653997	6171.185426	8.104909	-0.051733	4.247276
257.884526	6179.169432	8.109914	-0.051781	4.249925
258.178654	6187.238785	8.114918	-0.051841	4.252601
258.315447	6195.296895	8.119923	-0.051872	4.255270
258.395180	6203.272950	8.124928	-0.051892	4.257910
258.910347	6211.318765	8.129933	-0.051993	4.260575
259.201994	6219.281305	8.134938	-0.052052	4.263208
259.438399	6227.300481	8.139942	-0.052102	4.265859
259.610107	6235.323615	8.144947	-0.052139	4.268508
259.748663	6243.349837	8.149952	-0.052170	4.271156
260.069414	6251.455014	8.154957	-0.052235	4.273831
260.083616	6259.463330	8.159962	-0.052242	4.276469
260.314450	6267.435014	8.164966	-0.052291	4.279095
260.382605	6275.455693	8.169971	-0.052308	4.281734
260.736894	6283.424758	8.174976	-0.052380	4.284357
261.038000	6291.499031	8.179981	-0.052441	4.287013
261.000121	6299.469871	8.184986	-0.052439	4.289630
261.271947	6307.571175	8.189990	-0.052495	4.292291
261.577050	6315.558739	8.194995	-0.052557	4.294913
261.586730	6323.527027	8.200000	-0.052564	4.297525
261.732220	6331.585574	8.205005	-0.052596	4.300166
262.067725	6339.547312	8.210010	-0.052664	4.302775
262.314434	6347.579122	8.215014	-0.052715	4.305405
262.447350	6355.622437	8.220019	-0.052745	4.308036
262.579688	6363.628692	8.225024	-0.052774	4.310653
263.066214	6371.713955	8.230029	-0.052870	4.313297
263.208346	6379.721346	8.235034	-0.052902	4.315911
263.427047	6387.671601	8.240038	-0.052948	4.318506
263.486029	6395.715587	8.245043	-0.052964	4.321128
263.746696	6403.696730	8.250048	-0.053018	4.323730
264.046733	6411.739478	8.255053	-0.053079	4.326351
264.117362	6419.719302	8.260058	-0.053097	4.328948
264.315681	6427.774176	8.265062	-0.053139	4.331568
264.690552	6435.768720	8.270067	-0.053214	4.334169
264.644348	6443.842574	8.275072	-0.053211	4.336791
264.892128	6451.822735	8.280077	-0.053262	4.339383
265.168522	6459.846648	8.285082	-0.053319	4.341987
265.340086	6467.828539	8.290086	-0.053356	4.344576
265.357429	6475.875299	8.295091	-0.053364	4.347183
265.468424	6483.864241	8.300096	-0.053390	4.349771
265.747302	6491.979106	8.305101	-0.053447	4.352399
265.756305	6500.005876	8.310106	-0.053454	4.354995
266.273184	6508.004239	8.315110	-0.053555	4.357583
266.393457	6515.962144	8.320115	-0.053583	4.360154
266.489069	6523.982354	8.325120	-0.053606	4.362744
266.594344	6531.958792	8.330125	-0.053631	4.365318
266.729318	6539.983009	8.335130	-0.053661	4.367906
266.991975	6548.001899	8.340134	-0.053715	4.370492
267.296094	6556.068518	8.345139	-0.053777	4.373092
267.428678	6564.086941	8.350144	-0.053807	4.375673
267.488666	6572.097886	8.355149	-0.053823	4.378250
267.515559	6580.073378	8.360154	-0.053833	4.380815
267.762962	6588.108931	8.365158	-0.053885	4.383398
267.948952	6596.130960	8.370163	-0.053924	4.385975
268.040200	6604.102993	8.375168	-0.053946	4.388533
268.498991	6612.162986	8.380173	-0.054037	4.391121
268.612166	6620.180212	8.385178	-0.054063	4.393691
268.829990	6628.268670	8.390182	-0.054109	4.396283
268.986392	6636.196211	8.395187	-0.054143	4.398822
269.189019	6644.202798	8.400192	-0.054186	4.401385
269.334193	6652.239486	8.405197	-0.054218	4.403956
269.549898	6660.222152	8.410202	-0.054264	4.406508
270.052635	6668.248995	8.415206	-0.054363	4.409074
270.124737	6676.302130	8.420211	-0.054381	4.411645
270.127204	6684.310171	8.425216	-0.054387	4.414200
270.449497	6692.401240	8.430221	-0.054452	4.416781
270.543140	6700.347731	8.435226	-0.054475	4.419314
270.557844	6708.422575	8.440230	-0.054483	4.421885
270.739423	6716.357413	8.445235	-0.054522	4.424412
270.998416	6724.375268	8.450240	-0.054575	4.426963
271.061287	6732.445846	8.455245	-0.054592	4.429529
271.052482	6740.463171	8.460250	-0.054595	4.432077
271.456982	6748.525599	8.465254	-0.054676	4.434638
271.718541	6756.543644	8.470259	-0.054730	4.437184
271.819262	6764.474051	8.475264	-0.054754	4.439700
272.184140	6772.531594	8.480269	-0.054827	4.442256
272.426299	6780.433874	8.485274	-0.054877	4.444760
272.670034	6788.522176	8.490278	-0.054928	4.447322
272.817956	6796.529617	8.495283	-0.054960	4.449856
273.157659	6804.609401	8.500288	-0.055029	4.452413
273.462026	6812.612399	8.505293	-0.055091	4.454944
273.683660	6820.652715	8.510298	-0.055137	4.457484
274.002586	6828.643137	8.515302	-0.055202	4.460008
274.214414	6836.663230	8.520307	-0.055246	4.462539
274.256585	6844.637438	8.525312	-0.055259	4.465054
274.480534	6852.720128	8.530317	-0.055306	4.467602
274.742510	6860.656406	8.535322	-0.055360	4.470103
274.887174	6868.726492	8.540326	-0.055392	4.472644
275.029322	6876.759571	8.545331	-0.055424	4.475172
275.221751	6884.738130	8.550336	-0.055465	4.477682
275.382165	6892.754371	8.555341	-0.055500	4.480201
275.451540	6900.748284	8.560346	-0.055518	4.482712
275.721084	6908.760633	8.565351	-0.055573	4.485228
276.008872	6916.762487	8.570355	-0.055632	4.487740
276.130190	6924.788466	8.575360	-0.055660	4.490257
276.231180	6932.874005	8.580365	-0.055684	4.492791
276.396949	6940.834936	8.585370	-0.055720	4.495285
276.684345	6948.874089	8.590375	-0.055779	4.497802
276.707778	6956.932170	8.595379	-0.055788	4.500323
276.800383	6964.883327	8.600384	-0.055811	4.502809
277.102550	6972.849151	8.605389	-0.055872	4.505299
277.061603	6980.895320	8.610394	-0.055870	4.507812
277.410969	6988.923829	8.615399	-0.055940	4.510319
277.502786	6997.003013	8.620403	-0.055962	4.512840
277.675147	7005.049084	8.625408	-0.055999	4.515349
277.937570	7013.044921	8.630413	-0.056053	4.517841
278.140296	7020.963496	8.635418	-0.056096	4.520308
278.333444	7029.020985	8.640423	-0.056137	4.522817
278.472321	7037.008117	8.645427	-0.056168	4.525302
278.513077	7045.049570	8.650432	-0.056181	4.527802
278.782745	7053.063864	8.655437	-0.056237	4.530293
278.699002	7061.076855	8.660442	-0.056226	4.532782
279.029176	7069.079636	8.665447	-0.056293	4.535267
279.161957	7077.109243	8.670451	-0.056323	4.537758
279.363429	7085.086531	8.675456	-0.056365	4.540232
279.551475	7093.134839	8.680461	-0.056406	4.542726
279.668369	7101.085187	8.685466	-0.056432	4.545189
279.897292	7109.198721	8.690471	-0.056480	4.547701
279.977621	7117.191395	8.695475	-0.056500	4.550174
280.120094	7125.258859	8.700480	-0.056532	4.552669
280.552703	7133.284030	8.705485	-0.056618	4.555149
280.689548	7141.297843	8.710490	-0.056649	4.557625
280.865643	7149.212729	8.715495	-0.056686	4.560068
281.289997	7157.306062	8.720499	-0.056771	4.562566
281.409561	7165.242096	8.725504	-0.056798	4.565013
281.698608	7173.325727	8.730509	-0.056857	4.567505
281.826298	7181.275538	8.735514	-0.056886	4.569954
282.078648	7189.349989	8.740519	-0.056938	4.572440
282.175762	7197.367489	8.745523	-0.056962	4.574907
282.373115	7205.384008	8.750528	-0.057003	4.577372
282.808449	7213.409404	8.755533	-0.057090	4.579839
282.859646	7221.454447	8.760538	-0.057104	4.582311
282.961926	7229.395934	8.765543	-0.057129	4.584749
283.192769	7237.447280	8.770547	-0.057177	4.587220
283.388030	7245.455271	8.775552	-0.057218	4.589676
283.570961	7253.550177	8.780557	-0.057258	4.592157
283.713726	7261.519121	8.785562	-0.057289	4.594599
284.046324	7269.577810	8.790567	-0.057356	4.597066
284.076774	7277.524939	8.795571	-0.057367	4.599498
284.211358	7285.578309	8.800576	-0.057397	4.601962
284.570310	7293.532739	8.805581	-0.057469	4.604393
284.733176	7301.551907	8.810586	-0.057505	4.606843
284.945859	7309.567223	8.815591	-0.057550	4.609291
285.323511	7317.620652	8.820595	-0.057625	4.611749
285.188093	7325.622140	8.825600	-0.057605	4.614190
285.427841	7333.696583	8.830605	-0.057655	4.616652
285.581240	7341.628837	8.835610	-0.057689	4.619069
285.808478	7349.722251	8.840615	-0.057736	4.621533
285.920770	7357.677369	8.845619	-0.057762	4.623955
285.939851	7365.699217	8.850624	-0.057771	4.626395
286.200002	7373.737961	8.855629	-0.057825	4.628840
286.340660	7381.732585	8.860634	-0.057856	4.631269
286.501678	7389.763376	8.865639	-0.057891	4.633708
286.618514	7397.819986	8.870643	-0.057918	4.636154
286.852018	7405.777200	8.875648	-0.057967	4.638568
287.119770	7413.814939	8.880653	-0.058022	4.641006
287.195186	7421.789563	8.885658	-0.058041	4.643423
287.454720	7429.787431	8.890663	-0.058095	4.645845
287.594722	7437.864528	8.895667	-0.058126	4.648291
287.672796	7445.828109	8.900672	-0.058145	4.650701
288.060995	7453.914578	8.905677	-0.058223	4.653146
288.171594	7461.874334	8.910682	-0.058249	4.655552
288.379671	7469.918200	8.915687	-0.058293	4.657982
288.582982	7477.893950	8.920691	-0.058336	4.660391
288.777659	7485.926643	8.925696	-0.058377	4.662815
288.902977	7493.917756	8.930701	-0.058406	4.665226
288.785482	7501.985513	8.935706	-0.058389	4.667658
289.150952	7509.978858	8.940711	-0.058462	4.670067
289.221999	7518.048665	8.945715	-0.058481	4.672497
289.278305	7526.086328	8.950720	-0.058496	4.674917
289.761486	7534.131458	8.955725	-0.058591	4.677336
289.611973	7542.020709	8.960730	-0.058569	4.679709
289.761060	7550.092217	8.965735	-0.058602	4.682135
289.834518	7558.027203	8.970739	-0.058620	4.684519
290.072907	7566.085822	8.975744	-0.058670	4.686938
290.289748	7574.043472	8.980749	-0.058716	4.689326
290.139765	7582.082046	8.985754	-0.058693	4.691737
290.370143	7590.161589	8.990759	-0.058741	4.694159
290.771783	7598.210089	8.995763	-0.058821	4.696570
290.735690	7606.134699	9.000768	-0.058819	4.698943
290.863468	7614.193851	9.005773	-0.058848	4.701355
291.168693	7622.161434	9.010778	-0.058910	4.703738
291.352061	7630.199099	9.015783	-0.058950	4.706141
291.702853	7638.231801	9.020787	-0.059020	4.708541
291.892365	7646.220417	9.025792	-0.059061	4.710927
292.187625	7654.340588	9.030797	-0.059121	4.713350
292.060049	7662.264785	9.035802	-0.059102	4.715715
292.345827	7670.302201	9.040807	-0.059161	4.718112
292.504803	7678.317572	9.045811	-0.059195	4.720501
292.626934	7686.268615	9.050816	-0.059223	4.722869
293.100932	7694.340172	9.055821	-0.059317	4.725272
293.179974	7702.371424	9.060826	-0.059337	4.727662
293.224979	7710.366566	9.065831	-0.059350	4.730040
293.523326	7718.413379	9.070835	-0.059411	4.732432
293.698228	7726.436893	9.075840	-0.059449	4.734816
294.092752	7734.475157	9.080845	-0.059527	4.737202
294.050650	7742.417414	9.085850	-0.059525	4.739560
294.345295	7750.458712	9.090855	-0.059585	4.741946
294.642956	7758.416819	9.095859	-0.059645	4.744305
294.568848	7766.506643	9.100864	-0.059637	4.746703
294.680889	7774.503526	9.105869	-0.059663	4.749072
294.872561	7782.541204	9.110874	-0.059703	4.751452
295.268326	7790.584281	9.115879	-0.059782	4.753831
295.323075	7798.580066	9.120883	-0.059798	4.756196
295.452093	7806.554337	9.125888	-0.059827	4.758554
295.710278	7814.571161	9.130893	-0.059880	4.760922
295.929990	7822.591611	9.135898	-0.059926	4.763290
296.155386	7830.567562	9.140903	-0.059973	4.765644
296.425175	7838.629596	9.145907	-0.060029	4.768022
296.494268	7846.561901	9.150912	-0.060047	4.770362
296.639118	7854.676024	9.155917	-0.060079	4.772753
296.619623	7862.686123	9.160922	-0.060081	4.775113
296.876362	7870.666780	9.165927	-0.060133	4.777463
297.039404	7878.688388	9.170931	-0.060169	4.779823
297.065648	7886.677115	9.175936	-0.060179	4.782174
297.499684	7894.676564	9.180941	-0.060265	4.784524
297.422846	7902.737675	9.185946	-0.060256	4.786894
297.441260	7910.732910	9.190951	-0.060265	4.789242
297.886077	7918.758514	9.195955	-0.060353	4.791597
297.928711	7926.802513	9.200960	-0.060366	4.793958
298.032991	7934.838649	9.205965	-0.060390	4.796314
298.130815	7942.788154	9.210970	-0.060414	4.798645
298.251885	7950.802665	9.215975	-0.060441	4.800993
298.267724	7958.852567	9.220979	-0.060449	4.803350
298.620698	7966.800817	9.225984	-0.060520	4.805676
298.858591	7974.881423	9.230989	-0.060570	4.808039
298.911437	7982.852068	9.235994	-0.060585	4.810370
299.119016	7990.259762	9.240999	-0.060628	4.812534
299.425964	7994.793643	9.246003	-0.060688	4.813858
299.390031	7997.230541	9.251008	-0.060683	4.814570
299.639473	7998.605844	9.256013	-0.060730	4.814971
299.758104	7999.008601	9.261018	-0.060753	4.815088
299.861426	7999.938064	9.266023	-0.060773	4.815359
299.858069	7999.946555	9.271027	-0.060772	4.815361
299.787922	7999.928286	9.276032	-0.060759	4.815356
299.979282	7999.933591	9.281037	-0.060794	4.815357
300.027518	7999.857427	9.286042	-0.060803	4.815334
300.000592	7999.908282	9.291047	-0.060798	4.815349
300.308876	7999.905905	9.296051	-0.060856	4.815347
300.297702	7999.880062	9.301056	-0.060853	4.815340
300.317593	7999.938107	9.306061	-0.060857	4.815356
300.339815	7999.883958	9.311066	-0.060861	4.815340
300.445209	7999.907078	9.316071	-0.060881	4.815347
300.687395	7999.949569	9.321075	-0.060926	4.815358
300.627955	7999.926132	9.326080	-0.060915	4.815351
300.886237	8000.010578	9.331085	-0.060963	4.815375
300.728933	7999.953451	9.336090	-0.060933	4.815359
300.802632	7999.922602	9.341095	-0.060947	4.815350
300.977676	7999.986427	9.346099	-0.060980	4.815367
300.910758	7999.951108	9.351104	-0.060967	4.815357
301.013584	7999.996634	9.356109	-0.060986	4.815370
300.920784	7999.938439	9.361114	-0.060969	4.815354
301.072071	7999.985837	9.366119	-0.060997	4.815367
300.974709	7999.995976	9.371123	-0.060979	4.815370
300.891624	7999.909082	9.376128	-0.060963	4.815345
301.041631	7999.940425	9.381133	-0.060991	4.815354
300.997546	7999.946103	9.386138	-0.060983	4.815355
301.034150	7999.967015	9.391143	-0.060990	4.815361
301.230196	7999.965986	9.396147	-0.061026	4.815360
301.174573	7999.929785	9.401152	-0.061016	4.815350
301.311770	7999.960916	9.406157	-0.061041	4.815358
301.320778	7999.924718	9.411162	-0.061043	4.815348
301.345044	7999.967873	9.416167	-0.061047	4.815360
301.282067	7999.966824	9.421171	-0.061036	4.815360
301.221713	7999.934821	9.426176	-0.061024	4.815351
301.507682	7999.998349	9.431181	-0.061078	4.815368
301.600984	7999.950722	9.436186	-0.061095	4.815354
301.273030	7999.951692	9.441191	-0.061034	4.815356
301.409339	7999.936846	9.446195	-0.061059	4.815351
301.563298	7999.909465	9.451200	-0.061088	4.815342
301.647469	8000.053023	9.456205	-0.061103	4.815384
301.623110	8000.044063	9.461210	-0.061099	4.815381
301.772903	8000.024096	9.466215	-0.061127	4.815375
301.638248	8000.007962	9.471219	-0.061101	4.815370
301.531298	7999.958083	9.476224	-0.061081	4.815356
301.679872	7999.987265	9.481229	-0.061109	4.815364
301.553491	7999.942408	9.486234	-0.061085	4.815352
301.606353	7999.951832	9.491239	-0.061095	4.815354
301.539671	7999.998823	9.496243	-0.061083	4.815368
301.842891	7999.953608	9.501248	-0.061139	4.815354
301.845815	8000.054132	9.506253	-0.061140	4.815383
301.611024	7999.957236	9.511258	-0.061096	4.815356
301.760608	7999.967195	9.516263	-0.061124	4.815358
301.648643	7999.972817	9.521267	-0.061103	4.815360
301.748932	7999.919961	9.526272	-0.061121	4.815344
301.839884	7999.989876	9.531277	-0.061138	4.815364
301.788572	7999.964435	9.536282	-0.061129	4.815357
301.857646	7999.952749	9.541287	-0.061142	4.815353
301.877088	7999.996893	9.546291	-0.061145	4.815366
301.890171	8000.001382	9.551296	-0.061148	4.815367
301.874382	7999.984013	9.556301	-0.061145	4.815362
301.863896	8000.023385	9.561306	-0.061143	4.815374
301.985439	8000.051051	9.566311	-0.061165	4.815381
302.219077	8000.028199	9.571315	-0.061209	4.815374
301.890625	8000.006712	9.576320	-0.061147	4.815369
301.858740	8000.074591	9.581325	-0.061141	4.815389
302.050901	8000.015776	9.586330	-0.061177	4.815371
302.188394	8000.007363	9.591335	-0.061203	4.815368
302.163443	8000.017634	9.596339	-0.061198	4.815371
302.067245	7999.957243	9.601344	-0.061180	4.815354
302.179169	8000.015749	9.606349	-0.061201	4.815370
302.191396	8000.010602	9.611354	-0.061203	4.815369
302.120534	7999.986975	9.616359	-0.061190	4.815362
302.305712	8000.037076	9.621363	-0.061224	4.815376
302.175353	7999.953670	9.626368	-0.061200	4.815352
302.186262	8000.010500	9.631373	-0.061202	4.815369
302.113357	8000.031734	9.636378	-0.061188	4.815375
302.113192	7999.988969	9.641383	-0.061188	4.815363
302.258042	8000.049090	9.646387	-0.061215	4.815380
302.293842	8000.030439	9.651392	-0.061222	4.815374
302.228755	8000.011183	9.656397	-0.061210	4.815369
302.268031	8000.002210	9.661402	-0.061217	4.815366
302.322457	7999.998833	9.666407	-0.061227	4.815365
302.385027	8000.011625	9.671411	-0.061239	4.815368
302.274315	7999.980922	9.676416	-0.061218	4.815360
302.357951	8000.015443	9.681421	-0.061233	4.815369
302.393474	8000.030993	9.686426	-0.061240	4.815374
302.102409	7999.994091	9.691431	-0.061186	4.815364
302.061430	8000.040440	9.696435	-0.061178	4.815378
302.132749	7999.941139	9.701440	-0.061191	4.815349
302.326976	8000.010631	9.706445	-0.061227	4.815368
302.394414	7999.987160	9.711450	-0.061240	4.815361
302.377469	7999.985806	9.716455	-0.061237	4.815360
302.468103	8000.011891	9.721459	-0.061254	4.815368
302.392764	7999.942224	9.726464	-0.061239	4.815348
302.690323	7999.995259	9.731469	-0.061295	4.815362
302.591595	8000.013927	9.736474	-0.061276	4.815368
302.613705	8000.029254	9.741479	-0.061280	4.815372
302.487718	8000.081676	9.746483	-0.061257	4.815388
302.553700	8000.017561	9.751488	-0.061269	4.815369
302.575073	8000.004015	9.756493	-0.061273	4.815365
302.621153	8000.034705	9.761498	-0.061282	4.815374
302.580201	8000.006229	9.766503	-0.061274	4.815365
302.841795	8000.095013	9.771507	-0.061323	4.815390
302.678806	8000.037787	9.776512	-0.061292	4.815374
302.705467	8000.137638	9.781517	-0.061297	4.815403
302.657871	8000.060948	9.786522	-0.061288	4.815381
302.666355	8000.002292	9.791527	-0.061290	4.815364
302.552557	8000.120122	9.796531	-0.061269	4.815399
302.470808	8000.010797	9.801536	-0.061253	4.815367
302.653074	8000.017024	9.806541	-0.061287	4.815368
302.514737	8000.020069	9.811546	-0.061261	4.815370
302.611444	8000.032358	9.816551	-0.061279	4.815373
302.793531	8000.059962	9.821555	-0.061313	4.815380
302.760059	7999.989920	9.826560	-0.061307	4.815360
302.978215	7999.996742	9.831565	-0.061347	4.815361
302.879442	8000.058167	9.836570	-0.061329	4.815379
302.732837	7999.998007	9.841575	-0.061302	4.815362
302.833123	8000.006080	9.846579	-0.061320	4.815364
302.672686	8000.005552	9.851584	-0.061290	4.815365
302.943928	8000.069910	9.856589	-0.061341	4.815382
302.890023	8000.044425	9.861594	-0.061331	4.815375
302.850571	8000.006352	9.866599	-0.061323	4.815364
302.927474	8000.033279	9.871603	-0.061338	4.815372
302.748392	7999.977924	9.876608	-0.061304	4.815356
302.762928	7999.971748	9.881613	-0.061307	4.815355
302.637692	7999.988906	9.886618	-0.061283	4.815360
302.611092	7999.999150	9.891623	-0.061278	4.815363
302.668908	8000.097379	9.896627	-0.061289	4.815392
302.666689	8000.027856	9.901632	-0.061289	4.815371
302.895646	8000.040203	9.906637	-0.061331	4.815374
302.858637	7999.985068	9.911642	-0.061324	4.815358
302.744667	8000.024862	9.916647	-0.061303	4.815370
302.875153	8000.071919	9.921651	-0.061327	4.815383
302.850128	8000.013775	9.926656	-0.061323	4.815366
302.755662	8000.012204	9.931661	-0.061305	4.815366
302.885689	8000.026115	9.936666	-0.061329	4.815370
302.927506	8000.002219	9.941671	-0.061337	4.815363
302.812117	8000.102919	9.946675	-0.061315	4.815393
302.643601	8000.053085	9.951680	-0.061284	4.815379
303.013728	8000.068843	9.956685	-0.061353	4.815382
302.864803	8000.012920	9.961690	-0.061325	4.815366
302.763545	7999.968477	9.966695	-0.061306	4.815354
302.818738	8000.060249	9.971699	-0.061316	4.815380
303.049600	8000.044835	9.976704	-0.061359	4.815375
303.050925	8000.048060	9.981709	-0.061360	4.815375
302.925506	8000.042767	9.986714	-0.061336	4.815375
303.037251	8000.017893	9.991719	-0.061357	4.815367
302.964588	8000.044476	9.996723	-0.061343	4.815375
302.726692	7999.989214	10.001728	-0.061299	4.815360
302.977189	8000.014745	10.006733	-0.061346	4.815366
302.890871	8000.005826	10.011738	-0.061329	4.815364
302.797670	7999.964724	10.016743	-0.061312	4.815352
303.016317	8000.033554	10.021747	-0.061353	4.815371
303.004053	7999.989519	10.026752	-0.061350	4.815359
303.082678	8000.056026	10.031757	-0.061365	4.815378
302.929131	8000.048128	10.036762	-0.061336	4.815376
302.991232	8000.007465	10.041767	-0.061348	4.815364
303.212959	8000.034658	10.046771	-0.061389	4.815371
302.870495	8000.004384	10.051776	-0.061325	4.815364
303.007804	7999.981003	10.056781	-0.061351	4.815356
302.831144	7999.997309	10.061786	-0.061318	4.815362
303.015450	7999.989673	10.066791	-0.061352	4.815359
303.014508	8000.042032	10.071795	-0.061352	4.815374
303.050450	8000.027659	10.076800	-0.061358	4.815370
303.036850	8000.058429	10.081805	-0.061356	4.815379
303.112009	7999.999810	10.086810	-0.061370	4.815361
303.181157	7999.974229	10.091815	-0.061383	4.815353
303.357387	7999.998529	10.096819	-0.061415	4.815360
303.101448	7999.970760	10.101824	-0.061368	4.815353
303.170417	8000.026417	10.106829	-0.061381	4.815369
303.175769	8000.009398	10.111834	-0.061381	4.815364
303.021511	8000.017523	10.116839	-0.061353	4.815367
303.191312	8000.082337	10.121843	-0.061384	4.815385
303.056634	8000.012753	10.126848	-0.061359	4.815365
303.185553	8000.058715	10.131853	-0.061383	4.815378
303.217726	8000.050693	10.136858	-0.061389	4.815375
303.133186	8000.117699	10.141863	-0.061373	4.815395
303.328539	8000.134834	10.146867	-0.061410	4.815399
303.102824	7999.982498	10.151872	-0.061367	4.815356
303.251023	7999.998849	10.156877	-0.061395	4.815360
303.209801	8000.047333	10.161882	-0.061387	4.815375
303.408381	8000.018556	10.166887	-0.061424	4.815365
303.284694	8000.087050	10.171891	-0.061401	4.815386
303.319701	7999.980730	10.176896	-0.061408	4.815355
303.393389	8000.050363	10.181901	-0.061421	4.815375
303.396552	8000.052549	10.186906	-0.061422	4.815375
303.303868	8000.021075	10.191911	-0.061405	4.815366
303.329166	8000.098456	10.196915	-0.061409	4.815389
303.087378	8000.054887	10.201920	-0.061364	4.815377
303.311413	8000.036153	10.206925	-0.061406	4.815371
303.463317	8000.041877	10.211930	-0.061434	4.815372
303.261508	8000.012868	10.216935	-0.061396	4.815364
303.197345	8000.028902	10.221939	-0.061384	4.815369
303.099493	7999.977032	10.226944	-0.061366	4.815355
303.249702	8000.003038	10.231949	-0.061394	4.815361
303.017123	8000.045139	10.236954	-0.061351	4.815375
303.246914	7999.991224	10.241959	-0.061393	4.815358
303.288485	8000.030393	10.246963	-0.061401	4.815369
303.101975	8000.061499	10.251968	-0.061366	4.815379
303.471092	8000.081518	10.256973	-0.061435	4.815383
303.502023	8000.069200	10.261978	-0.061441	4.815380
303.235123	8000.029489	10.266983	-0.061391	4.815369
303.502413	8000.100198	10.271987	-0.061441	4.815389
303.341059	7999.987412	10.276992	-0.061411	4.815356
303.409014	8000.003501	10.281997	-0.061423	4.815361
303.266077	7999.988296	10.287002	-0.061397	4.815357
303.314586	7999.983752	10.292007	-0.061406	4.815355
303.433206	8000.038096	10.297011	-0.061428	4.815371
303.340776	8000.016247	10.302016	-0.061410	4.815365
303.376239	8000.018969	10.307021	-0.061417	4.815365
303.557428	8000.048697	10.312026	-0.061451	4.815373
303.383511	7999.984874	10.317031	-0.061418	4.815355
303.261962	8000.041646	10.322035	-0.061395	4.815373
303.566870	8000.060599	10.327040	-0.061452	4.815377
303.560471	8000.055144	10.332045	-0.061451	4.815375
303.270428	8000.070635	10.337050	-0.061397	4.815381
303.441310	8000.028571	10.342055	-0.061429	4.815368
303.579225	8000.063994	10.347059	-0.061454	4.815378
303.672003	7999.978943	10.352064	-0.061472	4.815352
303.558141	8000.055083	10.357069	-0.061450	4.815375
303.486242	8000.065644	10.362074	-0.061437	4.815379
303.542614	8000.015265	10.367079	-0.061447	4.815364
303.502776	8000.064841	10.372083	-0.061440	4.815378
303.384543	7999.990184	10.377088	-0.061418	4.815357
303.488159	8000.034658	10.382093	-0.061437	4.815370
303.516253	8000.046879	10.387098	-0.061442	4.815373
303.507054	7999.987929	10.392103	-0.061440	4.815356
303.695810	8000.056265	10.397107	-0.061476	4.815375
303.674643	8000.033461	10.402112	-0.061472	4.815368
303.655816	8000.016040	10.407117	-0.061468	4.815363
303.550886	8000.039949	10.412122	-0.061448	4.815371
303.696750	7999.997469	10.417127	-0.061475	4.815358
303.602670	8000.065387	10.422131	-0.061458	4.815378
303.305584	8000.019830	10.427136	-0.061403	4.815366
303.647647	8000.037262	10.432141	-0.061466	4.815370
303.493786	8000.014393	10.437146	-0.061438	4.815364
303.337683	7999.988281	10.442151	-0.061408	4.815357
303.509504	8000.029611	10.447155	-0.061440	4.815368
303.461418	8000.048050	10.452160	-0.061431	4.815374
303.613895	8000.062336	10.457165	-0.061460	4.815377
303.504778	8000.017761	10.462170	-0.061439	4.815365
303.482339	7999.946832	10.467175	-0.061435	4.815344
303.536211	8000.026826	10.472179	-0.061445	4.815367
303.527798	7999.967889	10.477184	-0.061443	4.815350
303.649689	8000.008390	10.482189	-0.061466	4.815361
303.542031	8000.025840	10.487194	-0.061446	4.815367
303.322734	7999.955920	10.492199	-0.061405	4.815347
303.738133	8000.016259	10.497203	-0.061482	4.815363
303.611828	7999.994917	10.502208	-0.061459	4.815357
303.609103	8000.024798	10.507213	-0.061458	4.815366
303.476375	7999.959522	10.512218	-0.061434	4.815348
303.598752	7999.950859	10.517223	-0.061456	4.815345
303.488296	8000.056987	10.522227	-0.061436	4.815376
303.480598	7999.980958	10.527232	-0.061434	4.815354
303.633722	8000.072220	10.532237	-0.061463	4.815380
303.537101	8000.080233	10.537242	-0.061445	4.815383
303.348619	8000.038617	10.542247	-0.061409	4.815371
303.395855	8000.053293	10.547251	-0.061418	4.815375
303.629954	8000.048623	10.552256	-0.061462	4.815373
303.395358	8000.000897	10.557261	-0.061418	4.815360
303.423905	8000.003504	10.562266	-0.061423	4.815361
303.526002	7999.980608	10.567271	-0.061442	4.815354
303.706401	8000.078737	10.572275	-0.061476	4.815381
303.702270	8000.016663	10.577280	-0.061475	4.815363
303.813142	8000.068741	10.582285	-0.061496	4.815378
303.789505	8000.070483	10.587290	-0.061491	4.815379
303.390622	8000.014684	10.592295	-0.061417	4.815364
303.556945	8000.069820	10.597299	-0.061448	4.815380
303.489137	8000.041966	10.602304	-0.061435	4.815372
303.488288	8000.090051	10.607309	-0.061435	4.815386
303.447032	8000.140673	10.612314	-0.061427	4.815401
303.591152	8000.050060	10.617319	-0.061454	4.815374
303.522707	8000.114127	10.622323	-0.061441	4.815393
303.458870	8000.074580	10.627328	-0.061429	4.815381
303.643292	8000.026326	10.632333	-0.061463	4.815366
303.569357	8000.094578	10.637338	-0.061450	4.815387
303.490782	8000.036613	10.642343	-0.061435	4.815370
303.580154	8000.063748	10.647347	-0.061452	4.815378
303.640733	8000.016645	10.652352	-0.061463	4.815364
303.682142	8000.049398	10.657357	-0.061470	4.815373
303.491168	8000.083637	10.662362	-0.061435	4.815384
303.482340	8000.031107	10.667367	-0.061433	4.815369
303.531425	8000.063986	10.672371	-0.061442	4.815378
303.554138	8000.026945	10.677376	-0.061446	4.815367
303.489773	8000.033355	10.682381	-0.061434	4.815369
303.453797	8000.004960	10.687386	-0.061428	4.815361
303.636988	7999.994100	10.692391	-0.061462	4.815357
303.534832	8000.041573	10.697395	-0.061443	4.815371
303.663661	8000.030879	10.702400	-0.061467	4.815368
303.629474	8000.015342	10.707405	-0.061460	4.815363
303.575344	8000.024060	10.712410	-0.061450	4.815366
303.666367	8000.036256	10.717415	-0.061467	4.815369
303.835120	8000.086088	10.722419	-0.061498	4.815383
303.719539	8000.009337	10.727424	-0.061477	4.815361
303.670159	8000.030961	10.732429	-0.061467	4.815368
303.786518	8000.042509	10.737434	-0.061489	4.815370
303.760519	7999.985417	10.742439	-0.061484	4.815354
303.854259	8000.044694	10.747443	-0.061502	4.815371
303.777716	7999.989970	10.752448	-0.061487	4.815355
303.876579	8000.015124	10.757453	-0.061506	4.815362
303.751033	8000.061140	10.762458	-0.061482	4.815376
303.807918	8000.051390	10.767463	-0.061493	4.815373
303.637586	8000.071006	10.772467	-0.061461	4.815380
303.528028	8000.085218	10.777472	-0.061441	4.815384
303.568730	8000.073062	10.782477	-0.061448	4.815380
303.802185	8000.065174	10.787482	-0.061492	4.815377
303.660974	8000.036101	10.792487	-0.061465	4.815369
303.505664	8000.067726	10.797491	-0.061436	4.815379
303.522722	8000.029522	10.802496	-0.061439	4.815368
303.733337	8000.005220	10.807501	-0.061479	4.815360
303.741518	8000.033145	10.812506	-0.061480	4.815368
303.637109	7999.998269	10.817511	-0.061460	4.815358
303.765459	8000.064534	10.822515	-0.061484	4.815377
303.670428	8000.037297	10.827520	-0.061467	4.815370
303.704271	8000.053889	10.832525	-0.061473	4.815374
303.785792	7999.996444	10.837530	-0.061488	4.815357
303.752638	7999.970234	10.842535	-0.061482	4.815350
303.952606	8000.068688	10.847539	-0.061519	4.815377
303.758252	7999.983146	10.852544	-0.061483	4.815353
303.977542	8000.025265	10.857549	-0.061524	4.815365
303.716203	8000.005957	10.862554	-0.061475	4.815360
303.641640	7999.976922	10.867559	-0.061461	4.815352
303.811938	8000.124056	10.872563	-0.061493	4.815394
303.728460	8000.089527	10.877568	-0.061477	4.815385
303.847323	8000.066910	10.882573	-0.061499	4.815377
303.712944	8000.068950	10.887578	-0.061474	4.815379
303.608341	8000.014830	10.892583	-0.061454	4.815363
303.853229	8000.086236	10.897587	-0.061500	4.815383
303.920645	8000.054213	10.902592	-0.061512	4.815373
303.987581	8000.054251	10.907597	-0.061525	4.815373
303.848432	8000.094696	10.912602	-0.061499	4.815385
303.680293	8000.056624	10.917607	-0.061468	4.815375
303.918647	8000.041335	10.922611	-0.061512	4.815370
303.815252	8000.008613	10.927616	-0.061493	4.815360
303.802229	8000.009462	10.932621	-0.061490	4.815361
304.095573	8000.046397	10.937626	-0.061545	4.815370
304.061316	8000.081100	10.942631	-0.061538	4.815380
303.827375	8000.115695	10.947635	-0.061495	4.815392
303.812252	8000.035266	10.952640	-0.061492	4.815368
303.791369	8000.035984	10.957645	-0.061488	4.815369
303.948509	8000.050347	10.962650	-0.061517	4.815372
303.958962	8000.005619	10.967655	-0.061519	4.815359
304.032669	8000.032494	10.972659	-0.061533	4.815366
303.883774	8000.050329	10.977664	-0.061505	4.815372
303.805689	8000.031924	10.982669	-0.061490	4.815367
303.890200	8000.033323	10.987674	-0.061506	4.815367
303.814072	7999.987158	10.992679	-0.061492	4.815354
303.842810	8000.025045	10.997683	-0.061497	4.815365
303.956748	7999.994862	11.002688	-0.061518	4.815356
304.256728	8000.029770	11.007693	-0.061574	4.815365
304.028445	8000.042010	11.012698	-0.061531	4.815369
303.800095	7999.991180	11.017703	-0.061489	4.815355
304.035085	8000.076319	11.022707	-0.061533	4.815379
304.029206	8000.042010	11.027712	-0.061531	4.815369
304.221779	8000.030237	11.032717	-0.061567	4.815365
304.243122	8000.085105	11.037722	-0.061571	4.815381
304.010988	8000.022453	11.042727	-0.061528	4.815364
304.024727	8000.056884	11.047731	-0.061530	4.815374
304.096256	8000.092275	11.052736	-0.061544	4.815384
304.316623	8000.140827	11.057741	-0.061585	4.815397
304.234179	8000.148006	11.062746	-0.061569	4.815399
303.945707	8000.036313	11.067751	-0.061516	4.815368
304.033077	8000.096553	11.072755	-0.061532	4.815385
304.227828	8000.076265	11.077760	-0.061568	4.815378
304.054200	8000.049860	11.082765	-0.061536	4.815371
304.151925	8000.108134	11.087770	-0.061554	4.815388
304.223027	8000.048378	11.092775	-0.061567	4.815370
304.294092	8000.036726	11.097779	-0.061580	4.815366
304.164639	8000.038848	11.102784	-0.061556	4.815368
304.321094	8000.054269	11.107789	-0.061585	4.815371
304.243518	8000.085047	11.112794	-0.061571	4.815381
304.084301	8000.035363	11.117799	-0.061541	4.815367
304.188965	8000.049924	11.122803	-0.061560	4.815371
304.191293	8000.028579	11.127808	-0.061561	4.815365
304.193876	8000.084205	11.132813	-0.061561	4.815381
304.228022	8000.104009	11.137818	-0.061567	4.815386
304.015554	8000.006407	11.142823	-0.061528	4.815359
304.210040	8000.062011	11.147827	-0.061564	4.815374
304.170026	8000.012169	11.152832	-0.061556	4.815360
304.345489	8000.023630	11.157837	-0.061589	4.815362
304.339917	8000.096225	11.162842	-0.061588	4.815384
304.185393	8000.000653	11.167847	-0.061559	4.815356
304.225343	8000.121038	11.172851	-0.061567	4.815391
304.188047	8000.118277	11.177856	-0.061560	4.815391
304.132345	8000.089554	11.182861	-0.061549	4.815383
304.058377	8000.070148	11.187866	-0.061535	4.815377
304.143064	7999.983893	11.192871	-0.061551	4.815352
304.163846	8000.034476	11.197875	-0.061555	4.815366
304.277454	8000.060945	11.202880	-0.061576	4.815374
304.367912	8000.062443	11.207885	-0.061593	4.815374
304.353968	8000.139174	11.212890	-0.061590	4.815396
304.087015	8000.091977	11.217895	-0.061540	4.815384
304.091296	8000.148701	11.222899	-0.061541	4.815400
304.075298	8000.093912	11.227904	-0.061538	4.815384
304.104474	8000.036667	11.232909	-0.061543	4.815367
303.987457	8000.071065	11.237914	-0.061522	4.815378
304.124724	7999.999580	11.242919	-0.061547	4.815356
304.261105	8000.069186	11.247923	-0.061573	4.815376
304.084056	8000.039518	11.252928	-0.061539	4.815368
304.073955	8000.021173	11.257933	-0.061538	4.815363
304.171887	8000.028139	11.262938	-0.061556	4.815365
304.052029	8000.028283	11.267943	-0.061533	4.815365
304.165383	8000.082541	11.272947	-0.061554	4.815380
304.300405	8000.113641	11.277952	-0.061580	4.815389
304.261159	8000.046708	11.282957	-0.061572	4.815370
304.152319	8000.035276	11.287962	-0.061552	4.815367
304.163378	8000.034386	11.292967	-0.061554	4.815366
304.111209	8000.021756	11.297971	-0.061544	4.815363
304.085622	8000.026672	11.302976	-0.061539	4.815365
304.118451	8000.011178	11.307981	-0.061545	4.815360
304.272298	8000.105661	11.312986	-0.061574	4.815387
304.143982	7999.984869	11.317991	-0.061550	4.815352
304.144491	8000.041529	11.322995	-0.061550	4.815369
304.254417	7999.952486	11.328000	-0.061570	4.815342
304.402433	7999.991285	11.333005	-0.061598	4.815353
304.402770	8000.089633	11.338010	-0.061598	4.815381
304.277609	8000.025549	11.343015	-0.061575	4.815363
304.502659	8000.098766	11.348019	-0.061617	4.815384
304.394912	8000.111939	11.353024	-0.061596	4.815388
304.346182	8000.104711	11.358029	-0.061587	4.815386
304.504010	8000.109466	11.363034	-0.061617	4.815387
304.350228	8000.049182	11.368039	-0.061588	4.815370
304.150006	8000.090750	11.373043	-0.061551	4.815383
304.085307	8000.065085	11.378048	-0.061539	4.815376
304.253716	8000.033669	11.383053	-0.061570	4.815366
304.111119	8000.033435	11.388058	-0.061543	4.815366
303.987523	7999.993965	11.393063	-0.061520	4.815355
304.205656	8000.111964	11.398067	-0.061561	4.815389
304.185062	8000.075272	11.403072	-0.061557	4.815378
304.395876	8000.039215	11.408077	-0.061596	4.815367
304.367179	8000.079356	11.413082	-0.061591	4.815379
304.257284	8000.032629	11.418087	-0.061570	4.815365
304.237382	8000.097503	11.423091	-0.061566	4.815385
304.151902	8000.073630	11.428096	-0.061550	4.815378
304.275446	8000.038263	11.433101	-0.061573	4.815367
304.267468	8000.102265	11.438106	-0.061572	4.815386
304.202728	8000.035978	11.443111	-0.061560	4.815367
304.349558	8000.129276	11.448115	-0.061587	4.815393
304.301880	8000.061133	11.453120	-0.061578	4.815374
304.105434	8000.004418	11.458125	-0.061541	4.815358
304.233480	8000.082437	11.463130	-0.061565	4.815380
304.085098	8000.043624	11.468135	-0.061538	4.815370
304.105210	8000.031125	11.473139	-0.061541	4.815366
304.157117	7999.991362	11.478144	-0.061551	4.815354
304.129603	7999.993038	11.483149	-0.061546	4.815355
304.228062	8000.066291	11.488154	-0.061564	4.815375
304.229327	8000.049204	11.493159	-0.061564	4.815370
304.376393	8000.090125	11.498163	-0.061592	4.815382
304.327966	8000.086109	11.503168	-0.061582	4.815381
304.046908	8000.049369	11.508173	-0.061530	4.815371
304.218943	8000.052221	11.513178	-0.061562	4.815371
304.238127	8000.087811	11.518183	-0.061566	4.815382
304.323746	8000.079608	11.523187	-0.061582	4.815379
304.425176	8000.089840	11.528192	-0.061600	4.815381
304.517273	8000.079606	11.533197	-0.061617	4.815378
304.367626	8000.125221	11.538202	-0.061590	4.815392
304.396461	8000.082936	11.543207	-0.061595	4.815380
304.269044	8000.147093	11.548211	-0.061571	4.815399
304.238809	8000.042895	11.553216	-0.061565	4.815369
304.302359	8000.045015	11.558221	-0.061577	4.815369
304.307831	8000.121000	11.563226	-0.061578	4.815391
304.284418	8000.021190	11.568231	-0.061574	4.815362
304.432940	8000.057860	11.573235	-0.061601	4.815372
304.328059	8000.045424	11.578240	-0.061582	4.815369
304.514420	8000.042100	11.583245	-0.061616	4.815367
304.532776	8000.081954	11.588250	-0.061620	4.815379
304.379716	8000.024889	11.593255	-0.061591	4.815363
304.475447	8000.114132	11.598259	-0.061609	4.815388
304.506348	8000.057984	11.603264	-0.061615	4.815372
304.353950	8000.036207	11.608269	-0.061586	4.815366
304.428840	8000.076999	11.613274	-0.061600	4.815378
304.442324	8000.004527	11.618279	-0.061603	4.815356
304.395488	8000.055056	11.623283	-0.061594	4.815371
304.289604	7999.999844	11.628288	-0.061574	4.815356
304.344839	8000.034965	11.633293	-0.061584	4.815366
304.363599	8000.086584	11.638298	-0.061588	4.815381
304.194525	8000.001460	11.643303	-0.061556	4.815357
304.461265	8000.042230	11.648307	-0.061606	4.815367
304.438897	8000.063234	11.653312	-0.061602	4.815374
304.329705	8000.017588	11.658317	-0.061581	4.815361
304.553202	8000.040537	11.663322	-0.061623	4.815366
304.501257	8000.031118	11.668327	-0.061613	4.815364
304.532121	8000.112870	11.673331	-0.061619	4.815388
304.393813	8000.054981	11.678336	-0.061593	4.815371
304.309883	8000.067480	11.683341	-0.061577	4.815375
304.692357	8000.111242	11.688346	-0.061649	4.815386
304.322458	8000.022782	11.693351	-0.061580	4.815362
304.192065	8000.083683	11.698355	-0.061555	4.815381
304.374126	8000.103806	11.703360	-0.061589	4.815386
304.290109	8000.043612	11.708365	-0.061573	4.815369
304.311168	8000.059992	11.713370	-0.061577	4.815373
304.138587	8000.011156	11.718375	-0.061545	4.815360
304.266488	8000.078483	11.723379	-0.061569	4.815379
304.239647	8000.104758	11.728384	-0.061564	4.815387
304.579080	8000.035560	11.733389	-0.061627	4.815365
304.507308	8000.054675	11.738394	-0.061614	4.815371
304.459061	8000.014317	11.743399	-0.061605	4.815359
304.476029	8000.031698	11.748403	-0.061608	4.815364
304.689507	8000.035239	11.753408	-0.061647	4.815364
304.387163	8000.077249	11.758413	-0.061591	4.815378
304.430665	8000.081174	11.763418	-0.061599	4.815379
304.381389	8000.035454	11.768423	-0.061590	4.815366
304.538502	8000.079750	11.773427	-0.061619	4.815378
304.315557	8000.079250	11.778432	-0.061577	4.815379
304.303091	8000.033072	11.783437	-0.061575	4.815365
304.519338	8000.143558	11.788442	-0.061615	4.815397
304.493329	8000.119604	11.793447	-0.061610	4.815390
304.521434	8000.158550	11.798451	-0.061616	4.815401
304.600111	8000.135266	11.803456	-0.061630	4.815394
304.313387	8000.078119	11.808461	-0.061577	4.815379
304.370788	8000.137862	11.813466	-0.061587	4.815396
304.343072	8000.122432	11.818471	-0.061582	4.815391
304.466785	8000.106309	11.823475	-0.061605	4.815386
304.273621	8000.159753	11.828480	-0.061569	4.815403
304.368738	8000.124983	11.833485	-0.061587	4.815392
304.744479	8000.116253	11.838490	-0.061657	4.815388
304.575113	8000.017226	11.843495	-0.061625	4.815360
304.606576	8000.077608	11.848499	-0.061631	4.815377
304.528177	8000.096612	11.853504	-0.061616	4.815383
304.466843	8000.037864	11.858509	-0.061605	4.815366
304.624121	8000.132405	11.863514	-0.061634	4.815393
304.739305	8000.023138	11.868519	-0.061655	4.815360
304.743702	8000.069173	11.873523	-0.061656	4.815374
304.520738	8000.051569	11.878528	-0.061615	4.815370
304.530816	8000.038904	11.883533	-0.061617	4.815366
304.754167	8000.103542	11.888538	-0.061658	4.815384
304.614310	8000.046696	11.893543	-0.061632	4.815368
304.563690	8000.025540	11.898547	-0.061622	4.815362
304.647176	8000.117787	11.903552	-0.061638	4.815389
304.571651	8000.041699	11.908557	-0.061624	4.815367
304.606493	8000.109620	11.913562	-0.061630	4.815386
304.608888	8000.054067	11.918567	-0.061631	4.815370
304.629704	8000.169861	11.923571	-0.061635	4.815404
304.686394	8000.140866	11.928576	-0.061645	4.815395
304.594933	8000.066650	11.933581	-0.061628	4.815374
304.659924	8000.053828	11.938586	-0.061640	4.815370
304.515924	8000.012949	11.943591	-0.061613	4.815359
304.450829	8000.070658	11.948595	-0.061601	4.815376
304.460166	8000.037670	11.953600	-0.061603	4.815366
304.529771	8000.008890	11.958605	-0.061616	4.815357
304.542792	8000.061482	11.963610	-0.061618	4.815373
304.434415	7999.992332	11.968615	-0.061598	4.815353
304.547541	8000.051932	11.973619	-0.061619	4.815370
304.693787	8000.065046	11.978624	-0.061646	4.815373
304.647737	8000.040759	11.983629	-0.061637	4.815366
304.925936	8000.115929	11.988634	-0.061689	4.815387
304.671827	8000.059323	11.993639	-0.061642	4.815371
304.619329	8000.103345	11.998643	-0.061632	4.815385
304.543590	8000.163016	12.003648	-0.061618	4.815402
304.575794	8000.086578	12.008653	-0.061624	4.815380
304.570169	8000.129240	12.013658	-0.061623	4.815392
304.535403	8000.069864	12.018663	-0.061616	4.815375
304.497099	8000.062809	12.023667	-0.061609	4.815373
304.430387	7999.983661	12.028672	-0.061596	4.815350
304.405198	8000.024929	12.033677	-0.061592	4.815363
304.547035	8000.099971	12.038682	-0.061618	4.815384
304.478321	8000.016513	12.043687	-0.061605	4.815360
304.566234	8000.101351	12.048691	-0.061622	4.815384
304.586230	8000.047159	12.053696	-0.061625	4.815368
304.513781	8000.057711	12.058701	-0.061612	4.815372
304.684150	8000.102227	12.063706	-0.061643	4.815384
304.576515	8000.023467	12.068711	-0.061623	4.815361
304.534402	8000.064454	12.073715	-0.061615	4.815374
304.559139	8000.047757	12.078720	-0.061620	4.815369
304.414264	8000.040002	12.083725	-0.061593	4.815367
304.577126	8000.058737	12.088730	-0.061623	4.815372
304.716751	8000.024705	12.093735	-0.061649	4.815361
304.611698	8000.083889	12.098739	-0.061630	4.815379
304.651810	8000.023618	12.103744	-0.061637	4.815361
304.589967	8000.012966	12.108749	-0.061625	4.815358
304.577613	8000.151726	12.113754	-0.061623	4.815399
304.641410	8000.128194	12.118759	-0.061635	4.815392
304.660751	8000.096441	12.123763	-0.061638	4.815382
304.672398	8000.092354	12.128768	-0.061641	4.815381
304.608197	8000.036765	12.133773	-0.061628	4.815365
304.641961	8000.098254	12.138778	-0.061635	4.815383
304.597026	8000.047260	12.143783	-0.061626	4.815368
304.385966	8000.071545	12.148787	-0.061587	4.815376
304.598318	8000.052618	12.153792	-0.061626	4.815370
304.715219	8000.006450	12.158797	-0.061648	4.815356
304.622988	8000.100055	12.163802	-0.061631	4.815384
304.575950	8000.013750	12.168807	-0.061622	4.815359
304.718236	8000.042833	12.173811	-0.061649	4.815366
304.821587	8000.073408	12.178816	-0.061668	4.815375
304.637985	8000.022250	12.183821	-0.061634	4.815361
304.785346	8000.143352	12.188826	-0.061661	4.815395
304.694982	8000.077706	12.193831	-0.061644	4.815377
304.749913	8000.072200	12.198835	-0.061654	4.815375
304.713447	8000.079073	12.203840	-0.061647	4.815377
304.485191	8000.076347	12.208845	-0.061605	4.815377
304.645643	8000.154907	12.213850	-0.061635	4.815399
304.368189	8000.069051	12.218855	-0.061583	4.815376
304.729436	8000.144531	12.223859	-0.061650	4.815396
304.774566	8000.065101	12.228864	-0.061659	4.815373
304.675606	8000.082695	12.233869	-0.061640	4.815378
304.609799	8000.148945	12.238874	-0.061628	4.815398
304.753235	8000.119252	12.243879	-0.061654	4.815389
304.651468	8000.100454	12.248883	-0.061635	4.815384
304.858221	8000.101745	12.253888	-0.061674	4.815383
304.880612	8000.066836	12.258893	-0.061678	4.815373
304.815505	8000.120269	12.263898	-0.061666	4.815389
304.437938	8000.029544	12.268903	-0.061595	4.815364
304.643138	8000.062879	12.273907	-0.061634	4.815373
304.669054	8000.068650	12.278912	-0.061638	4.815374
304.713361	8000.074726	12.283917	-0.061647	4.815376
304.700678	8000.127961	12.288922	-0.061644	4.815391
304.651365	8000.033066	12.293927	-0.061635	4.815364
304.678707	8000.103001	12.298931	-0.061640	4.815384
304.655010	8000.121845	12.303936	-0.061636	4.815390
304.801129	8000.036609	12.308941	-0.061663	4.815364
304.678281	8000.120085	12.313946	-0.061640	4.815389
304.387934	8000.020118	12.318951	-0.061586	4.815361
304.771871	8000.050007	12.323955	-0.061657	4.815368
304.800808	8000.016275	12.328960	-0.061662	4.815358
304.594033	7999.983975	12.333965	-0.061624	4.815350
304.646468	8000.017980	12.338970	-0.061634	4.815360
304.536423	8000.051425	12.343975	-0.061613	4.815370
304.724033	8000.027811	12.348979	-0.061648	4.815362
304.655851	8000.061951	12.353984	-0.061635	4.815372
304.785308	8000.006371	12.358989	-0.061659	4.815355
304.713488	8000.076797	12.363994	-0.061646	4.815376
304.450599	7999.991183	12.368999	-0.061597	4.815353
304.709360	8000.028615	12.374003	-0.061645	4.815362
304.687711	8000.061390	12.379008	-0.061641	4.815372
304.601261	8000.022535	12.384013	-0.061625	4.815361
304.883495	8000.045390	12.389018	-0.061677	4.815366
304.840375	7999.999772	12.394023	-0.061669	4.815353
304.946738	8000.045363	12.399027	-0.061689	4.815366
304.745341	8000.093326	12.404032	-0.061651	4.815381
304.620061	8000.033515	12.409037	-0.061628	4.815364
304.753092	8000.057100	12.414042	-0.061653	4.815370
304.553454	8000.021710	12.419047	-0.061616	4.815361
304.827877	8000.052988	12.424051	-0.061667	4.815369
305.091469	8000.057362	12.429056	-0.061716	4.815369
304.981439	8000.011701	12.434061	-0.061695	4.815356
304.861046	8000.037491	12.439066	-0.061673	4.815364
304.884294	7999.997251	12.444071	-0.061677	4.815352
304.743558	8000.019496	12.449075	-0.061651	4.815360
304.687452	8000.008939	12.454080	-0.061640	4.815357
304.769616	7999.992126	12.459085	-0.061655	4.815351
305.027517	8000.028475	12.464090	-0.061703	4.815361
304.700087	8000.044413	12.469095	-0.061642	4.815367
304.775145	8000.029620	12.474099	-0.061656	4.815362
304.783880	8000.078935	12.479104	-0.061658	4.815377
304.666679	8000.016051	12.484109	-0.061636	4.815359
304.625296	8000.088051	12.489114	-0.061628	4.815380
304.696940	8000.045408	12.494119	-0.061642	4.815367
304.872807	8000.076118	12.499123	-0.061674	4.815375
304.794969	8000.076959	12.504128	-0.061660	4.815376
304.947068	7999.997168	12.509133	-0.061688	4.815352
304.872980	8000.064349	12.514138	-0.061674	4.815372
304.804644	8000.074969	12.519143	-0.061661	4.815375
304.880611	8000.062329	12.524147	-0.061675	4.815371
304.826897	8000.034708	12.529152	-0.061665	4.815364
304.817728	8000.004619	12.534157	-0.061664	4.815355
304.809053	8000.057921	12.539162	-0.061662	4.815370
304.920663	7999.996699	12.544167	-0.061683	4.815352
304.885182	8000.014278	12.549171	-0.061676	4.815357
304.788546	8000.086430	12.554176	-0.061658	4.815379
304.828631	7999.996226	12.559181	-0.061665	4.815352
305.055151	7999.993570	12.564186	-0.061707	4.815350
304.799504	8000.024597	12.569191	-0.061660	4.815361
304.896010	8000.027264	12.574195	-0.061678	4.815361
304.930960	8000.011805	12.579200	-0.061684	4.815356
304.857718	8000.002033	12.584205	-0.061671	4.815354
304.838059	8000.027358	12.589210	-0.061667	4.815361
304.773798	7999.973905	12.594215	-0.061655	4.815346
304.914580	8000.021137	12.599219	-0.061681	4.815359
304.775869	8000.056244	12.604224	-0.061655	4.815370
304.689228	7999.997075	12.609229	-0.061639	4.815353
304.782261	8000.026409	12.614234	-0.061656	4.815361
304.719295	7999.999703	12.619239	-0.061644	4.815354
304.726324	7999.997678	12.624243	-0.061646	4.815353
304.981380	8000.008323	12.629248	-0.061693	4.815355
304.971844	8000.008160	12.634253	-0.061691	4.815355
304.854296	7999.992307	12.639258	-0.061669	4.815351
304.529347	8000.010424	12.644263	-0.061609	4.815358
304.742570	8000.019306	12.649267	-0.061648	4.815360
304.804474	7999.997880	12.654272	-0.061660	4.815353
304.736373	7999.993538	12.659277	-0.061647	4.815352
305.023307	8000.035714	12.664282	-0.061701	4.815363
305.067120	7999.995815	12.669287	-0.061709	4.815351
304.886837	7999.999231	12.674291	-0.061675	4.815353
305.111075	8000.042504	12.679296	-0.061717	4.815365
304.964953	8000.016554	12.684301	-0.061690	4.815358
304.922739	8000.101369	12.689306	-0.061682	4.815383
304.756457	8000.019497	12.694311	-0.061651	4.815360
304.893069	8000.000382	12.699315	-0.061676	4.815353
304.981701	8000.089507	12.704320	-0.061693	4.815379
304.642097	8000.028275	12.709325	-0.061629	4.815363
304.881154	8000.006585	12.714330	-0.061674	4.815355
304.945468	8000.000165	12.719335	-0.061686	4.815353
304.922134	8000.102398	12.724339	-0.061681	4.815383
304.913156	8000.085140	12.729344	-0.061679	4.815378
304.930652	8000.064046	12.734349	-0.061683	4.815372
304.991556	8000.088572	12.739354	-0.061694	4.815379
304.850606	8000.037052	12.744359	-0.061668	4.815364
304.963706	8000.014339	12.749363	-0.061689	4.815357
304.952722	8000.031256	12.754368	-0.061687	4.815362
304.868350	8000.042679	12.759373	-0.061671	4.815366
304.931754	8000.064038	12.764378	-0.061683	4.815372
304.936499	8000.010663	12.769383	-0.061683	4.815356
304.833018	8000.002526	12.774387	-0.061664	4.815354
305.049071	8000.026421	12.779392	-0.061704	4.815360
304.851615	7999.996412	12.784397	-0.061667	4.815352
304.971630	8000.041161	12.789402	-0.061690	4.815365
304.863280	8000.009425	12.794407	-0.061670	4.815356
305.007352	8000.037469	12.799411	-0.061696	4.815364
305.164858	8000.059323	12.804416	-0.061726	4.815369
304.981005	8000.042368	12.809421	-0.061691	4.815365
305.056752	8000.070347	12.814426	-0.061705	4.815373
304.912333	8000.021977	12.819431	-0.061678	4.815360
305.018471	8000.079324	12.824435	-0.061698	4.815376
304.924133	8000.093787	12.829440	-0.061681	4.815380
304.889378	8000.016238	12.834445	-0.061674	4.815358
305.192879	8000.062965	12.839450	-0.061730	4.815370
305.016249	8000.025819	12.844455	-0.061698	4.815360
305.087160	7999.998129	12.849459	-0.061711	4.815352
305.042472	7999.981348	12.854464	-0.061702	4.815347
304.967018	7999.989711	12.859469	-0.061688	4.815350
305.071136	8000.025644	12.864474	-0.061708	4.815360
304.893675	8000.046211	12.869479	-0.061674	4.815367
304.949456	8000.104859	12.874483	-0.061685	4.815384
304.926770	8000.111961	12.879488	-0.061681	4.815386
305.075991	8000.038535	12.884493	-0.061708	4.815364
305.248527	8000.032845	12.889498	-0.061740	4.815361
305.073476	8000.008553	12.894503	-0.061708	4.815355
305.106642	8000.046514	12.899507	-0.061714	4.815366
305.280660	8000.044056	12.904512	-0.061746	4.815364
305.154245	8000.076160	12.909517	-0.061723	4.815374
305.199375	8000.094009	12.914522	-0.061731	4.815379
305.145941	8000.076013	12.919527	-0.061721	4.815374
305.077718	8000.077014	12.924531	-0.061708	4.815375
304.977167	8000.114892	12.929536	-0.061689	4.815386
305.108881	7999.983450	12.934541	-0.061714	4.815347
305.059534	8000.107700	12.939546	-0.061705	4.815384
304.856097	8000.034831	12.944551	-0.061667	4.815364
305.049980	8000.090428	12.949555	-0.061703	4.815379
305.164460	8000.092325	12.954560	-0.061724	4.815379
305.124608	8000.071348	12.959565	-0.061717	4.815373
305.097404	8000.104031	12.964570	-0.061712	4.815383
304.986296	8000.044455	12.969575	-0.061691	4.815366
304.899634	8000.051563	12.974579	-0.061675	4.815368
304.946874	8000.117553	12.979584	-0.061683	4.815387
305.032287	8000.048413	12.984589	-0.061699	4.815367
305.080860	8000.122977	12.989594	-0.061708	4.815388
304.916419	8000.024030	12.994599	-0.061677	4.815360
304.948795	8000.063048	12.999603	-0.061683	4.815371
305.041494	7999.992960	13.004608	-0.061701	4.815350
305.090412	7999.969181	13.009613	-0.061710	4.815343
305.036360	8000.060213	13.014618	-0.061700	4.815370
305.039160	8000.031392	13.019623	-0.061700	4.815362
305.175009	8000.020816	13.024627	-0.061725	4.815358
305.033625	8000.078328	13.029632	-0.061699	4.815375
304.915122	7999.998318	13.034637	-0.061677	4.815353
305.166601	8000.080528	13.039642	-0.061724	4.815375
304.956188	8000.084512	13.044647	-0.061684	4.815378
305.044505	8000.076353	13.049651	-0.061701	4.815375
305.091484	8000.067508	13.054656	-0.061710	4.815372
304.935010	8000.034973	13.059661	-0.061680	4.815363
304.956892	8000.070609	13.064666	-0.061684	4.815374
305.092772	8000.066447	13.069671	-0.061710	4.815372
305.181669	8000.079679	13.074675	-0.061726	4.815375
305.063978	8000.111928	13.079680	-0.061704	4.815385
305.048983	7999.995153	13.084685	-0.061701	4.815351
305.197605	8000.077792	13.089690	-0.061729	4.815375
305.105336	8000.062358	13.094695	-0.061712	4.815370
305.070199	8000.026493	13.099699	-0.061705	4.815360
305.140511	8000.057589	13.104704	-0.061718	4.815369
305.046106	7999.986531	13.109709	-0.061700	4.815349
305.052520	8000.107431	13.114714	-0.061702	4.815384
304.990255	8000.105323	13.119719	-0.061690	4.815384
305.131920	8000.064912	13.124723	-0.061716	4.815371
305.021246	8000.053448	13.129728	-0.061696	4.815368
304.799067	8000.020891	13.134733	-0.061654	4.815360
305.012859	8000.091784	13.139738	-0.061694	4.815380
305.007006	8000.012576	13.144743	-0.061693	4.815356
304.893032	8000.023507	13.149747	-0.061672	4.815360
305.144316	8000.049056	13.154752	-0.061718	4.815366
305.224257	8000.008688	13.159757	-0.061733	4.815354
305.256611	8000.054120	13.164762	-0.061739	4.815367
305.173776	7999.992875	13.169767	-0.061724	4.815350
305.388546	8000.016749	13.174771	-0.061764	4.815356
305.322709	8000.024203	13.179776	-0.061751	4.815358
305.016267	8000.024454	13.184781	-0.061694	4.815360
305.442998	8000.058263	13.189786	-0.061774	4.815368
305.371376	8000.019654	13.194791	-0.061760	4.815357
305.370437	8000.011082	13.199795	-0.061760	4.815354
305.390141	8000.062717	13.204800	-0.061764	4.815369
305.430765	8000.020627	13.209805	-0.061771	4.815357
305.307797	8000.055995	13.214810	-0.061748	4.815368
305.176518	8000.018533	13.219815	-0.061724	4.815357
305.238096	8000.045208	13.224819	-0.061735	4.815365
305.338336	8000.066111	13.229824	-0.061754	4.815370
305.147249	8000.042621	13.234829	-0.061718	4.815365
305.281037	8000.089738	13.239834	-0.061743	4.815378
305.370566	8000.057012	13.244839	-0.061760	4.815368
305.312967	8000.068879	13.249843	-0.061749	4.815371
305.233363	8000.013033	13.254848	-0.061734	4.815355
305.215590	7999.993491	13.259853	-0.061731	4.815350
305.241192	8000.156402	13.264858	-0.061735	4.815397
305.047875	8000.074079	13.269863	-0.061699	4.815374
305.186965	8000.028280	13.274867	-0.061725	4.815360
305.219098	8000.061949	13.279872	-0.061731	4.815370
305.263262	8000.078713	13.284877	-0.061739	4.815375
305.258270	8000.150250	13.289882	-0.061738	4.815395
305.202157	8000.074482	13.294887	-0.061728	4.815374
305.240165	8000.031280	13.299891	-0.061735	4.815361
305.277054	8000.098167	13.304896	-0.061742	4.815380
305.243443	8000.045223	13.309901	-0.061735	4.815365
305.309867	8000.101910	13.314906	-0.061748	4.815381
305.224492	8000.078038	13.319911	-0.061732	4.815375
305.315672	8000.067790	13.324915	-0.061749	4.815371
305.467719	8000.137659	13.329920	-0.061777	4.815391
305.421643	8000.105888	13.334925	-0.061768	4.815382
305.376910	8000.094450	13.339930	-0.061760	4.815379
305.305681	8000.123195	13.344935	-0.061747	4.815387
305.302609	8000.050447	13.349939	-0.061746	4.815366
305.535487	8000.087450	13.354944	-0.061789	4.815376
305.551239	8000.048154	13.359949	-0.061792	4.815364
305.533040	8000.030743	13.364954	-0.061789	4.815359
305.321101	8000.014390	13.369959	-0.061749	4.815355
305.451894	7999.996247	13.374963	-0.061773	4.815350
305.515897	8000.011203	13.379968	-0.061785	4.815354
305.059032	8000.001472	13.384973	-0.061700	4.815353
305.240034	8000.092133	13.389978	-0.061734	4.815379
305.323175	8000.013334	13.394983	-0.061749	4.815355
305.401773	8000.057395	13.399987	-0.061764	4.815368
305.241191	8000.083587	13.404992	-0.061734	4.815376
305.313951	8000.044169	13.409997	-0.061747	4.815364
305.471955	8000.058548	13.415002	-0.061777	4.815368
305.353733	8000.040545	13.420007	-0.061755	4.815363
305.476895	8000.076795	13.425011	-0.061778	4.815373
305.451661	8000.115925	13.430016	-0.061773	4.815385
305.422335	8000.066259	13.435021	-0.061767	4.815370
305.422553	8000.064120	13.440026	-0.061767	4.815370
305.315659	8000.087996	13.445031	-0.061747	4.815377
305.138370	8000.036941	13.450035	-0.061714	4.815363
305.292782	8000.059813	13.455040	-0.061743	4.815369
305.360385	8000.041689	13.460045	-0.061756	4.815363
305.326853	8000.086027	13.465050	-0.061749	4.815376
305.220573	8000.121672	13.470055	-0.061730	4.815387
305.167453	8000.133614	13.475059	-0.061720	4.815391
305.428172	8000.158252	13.480064	-0.061768	4.815397
305.268772	8000.056181	13.485069	-0.061738	4.815368
305.369742	8000.160479	13.490074	-0.061757	4.815398
305.456611	8000.102053	13.495079	-0.061773	4.815380
305.339534	8000.101173	13.500083	-0.061751	4.815381
305.280194	8000.101252	13.505088	-0.061740	4.815381
305.337985	7999.997444	13.510093	-0.061751	4.815350
305.361311	8000.054485	13.515098	-0.061755	4.815367
305.200164	8000.047528	13.520103	-0.061725	4.815366
305.217899	8000.055301	13.525107	-0.061728	4.815368
305.247359	8000.103892	13.530112	-0.061734	4.815382
305.150301	8000.087309	13.535117	-0.061716	4.815378
305.177212	8000.078131	13.540122	-0.061721	4.815375
305.304263	8000.021441	13.545127	-0.061744	4.815358
305.404317	8000.050893	13.550131	-0.061763	4.815366
305.317718	8000.039829	13.555136	-0.061747	4.815363
305.406495	8000.004953	13.560141	-0.061763	4.815352
305.430544	8000.095145	13.565146	-0.061768	4.815379
305.118540	8000.052543	13.570151	-0.061710	4.815368
305.303306	8000.063090	13.575155	-0.061744	4.815370
305.398775	8000.092466	13.580160	-0.061762	4.815378
305.261575	8000.062388	13.585165	-0.061736	4.815370
305.077071	8000.036870	13.590170	-0.061702	4.815363
305.408843	8000.038101	13.595175	-0.061763	4.815362
305.394701	7999.999377	13.600179	-0.061761	4.815351
305.299659	8000.065142	13.605184	-0.061743	4.815370
305.208801	7999.990936	13.610189	-0.061726	4.815349
305.201810	7999.997229	13.615194	-0.061725	4.815351
305.415307	8000.002909	13.620199	-0.061764	4.815352
305.229056	8000.057537	13.625203	-0.061730	4.815369
305.325482	8000.082653	13.630208	-0.061747	4.815375
305.247929	8000.047152	13.635213	-0.061733	4.815365
305.255867	8000.099661	13.640218	-0.061734	4.815381
305.200086	8000.063453	13.645223	-0.061724	4.815370
305.323616	8000.062293	13.650227	-0.061747	4.815370
305.315839	8000.105989	13.655232	-0.061745	4.815382
305.194451	8000.049449	13.660237	-0.061723	4.815366
305.357223	8000.078874	13.665242	-0.061753	4.815374
305.290455	8000.075622	13.670247	-0.061741	4.815374
305.160646	8000.022149	13.675251	-0.061716	4.815359
305.512571	8000.081441	13.680256	-0.061782	4.815374
305.344103	8000.047637	13.685261	-0.061750	4.815365
305.243886	8000.080176	13.690266	-0.061732	4.815375
305.458891	8000.119021	13.695271	-0.061772	4.815385
305.438813	8000.076992	13.700275	-0.061768	4.815373
305.342641	8000.091425	13.705280	-0.061750	4.815378
305.156150	8000.004940	13.710285	-0.061715	4.815354
305.388995	8000.059047	13.715290	-0.061758	4.815368
305.358329	8000.047843	13.720295	-0.061753	4.815365
305.428938	8000.054356	13.725299	-0.061766	4.815367
305.395952	8000.099772	13.730304	-0.061760	4.815380
305.338922	8000.038955	13.735309	-0.061749	4.815363
305.377027	8000.057757	13.740314	-0.061756	4.815368
305.463503	8000.006808	13.745319	-0.061772	4.815353
305.398397	8000.045275	13.750323	-0.061760	4.815364
305.598690	8000.073186	13.755328	-0.061797	4.815371
305.558419	8000.052201	13.760333	-0.061790	4.815365
305.553894	8000.079916	13.765338	-0.061789	4.815374
305.444194	8000.119781	13.770343	-0.061768	4.815386
305.340847	8000.065678	13.775347	-0.061749	4.815370
305.424891	8000.163281	13.780352	-0.061765	4.815399
305.277848	8000.056071	13.785357	-0.061737	4.815368
305.264413	8000.084706	13.790362	-0.061735	4.815376
305.212409	8000.062458	13.795367	-0.061725	4.815370
305.331874	8000.009918	13.800371	-0.061747	4.815354
305.418451	8000.049837	13.805376	-0.061763	4.815365
305.281708	8000.039009	13.810381	-0.061738	4.815363
305.495373	8000.086383	13.815386	-0.061777	4.815376
305.627734	8000.099268	13.820391	-0.061802	4.815379
305.279283	8000.125545	13.825395	-0.061737	4.815388
305.245048	8000.153836	13.830400	-0.061731	4.815397
305.235729	8000.016843	13.835405	-0.061729	4.815357
305.417607	8000.104312	13.840410	-0.061763	4.815381
305.382297	8000.087686	13.845415	-0.061756	4.815377
305.510205	8000.018182	13.850419	-0.061780	4.815356
305.475132	8000.046458	13.855424	-0.061773	4.815364
305.437816	8000.034075	13.860429	-0.061766	4.815361
305.385782	8000.087726	13.865434	-0.061756	4.815377
305.389476	8000.087783	13.870439	-0.061757	4.815377
305.438663	8000.091803	13.875443	-0.061766	4.815378
305.529843	8000.074071	13.880448	-0.061783	4.815372
305.435362	8000.001942	13.885453	-0.061765	4.815351
305.334097	8000.101812	13.890458	-0.061747	4.815381
305.205617	8000.102880	13.895463	-0.061723	4.815382
305.601731	8000.044246	13.900467	-0.061796	4.815363
305.643965	8000.088773	13.905472	-0.061804	4.815376
305.404447	7999.987510	13.910477	-0.061759	4.815347
305.331437	8000.046157	13.915482	-0.061746	4.815365
305.607533	8000.011186	13.920487	-0.061797	4.815353
305.421588	8000.023059	13.925491	-0.061762	4.815358
305.302599	8000.029630	13.930496	-0.061740	4.815360
305.522087	8000.030065	13.935501	-0.061781	4.815359
305.559291	8000.089474	13.940506	-0.061788	4.815376
305.509558	8000.039469	13.945511	-0.061779	4.815362
305.554512	8000.055178	13.950515	-0.061787	4.815366
305.674931	8000.156593	13.955520	-0.061809	4.815395
305.353070	8000.078548	13.960525	-0.061749	4.815374
305.437420	8000.095980	13.965530	-0.061765	4.815379
305.537242	8000.071977	13.970535	-0.061784	4.815371
305.444344	8000.034083	13.975539	-0.061766	4.815361
305.356072	8000.044372	13.980544	-0.061750	4.815364
305.256124	8000.014913	13.985549	-0.061731	4.815356
305.380645	8000.022322	13.990554	-0.061754	4.815358
305.436737	8000.014697	13.995559	-0.061765	4.815355
305.403886	7999.999181	14.000563	-0.061758	4.815351
305.504033	8000.076740	14.005568	-0.061777	4.815373
305.473862	8000.014232	14.010573	-0.061771	4.815355
305.455128	8000.029952	14.015578	-0.061768	4.815360
305.584244	8000.064163	14.020583	-0.061792	4.815369
305.444728	8000.037253	14.025587	-0.061766	4.815362
305.492245	8000.061557	14.030592	-0.061775	4.815369
305.389696	8000.034192	14.035597	-0.061755	4.815361
305.335338	8000.055734	14.040602	-0.061745	4.815368
305.239084	8000.056269	14.045607	-0.061727	4.815368
305.056238	8000.051090	14.050611	-0.061693	4.815368
305.383260	8000.099278	14.055616	-0.061754	4.815380
305.146583	8000.017305	14.060621	-0.061710	4.815357
305.331541	8000.063133	14.065626	-0.061744	4.815370
305.335100	8000.086706	14.070631	-0.061745	4.815377
305.470088	8000.030148	14.075635	-0.061770	4.815360
305.236776	8000.094685	14.080640	-0.061727	4.815380
305.365302	8000.058331	14.085645	-0.061750	4.815368
305.441587	8000.014695	14.090650	-0.061765	4.815355
305.274395	8000.057881	14.095655	-0.061733	4.815369
305.370021	8000.027395	14.100659	-0.061751	4.815359
305.313186	8000.023239	14.105664	-0.061741	4.815358
305.317190	8000.054303	14.110669	-0.061741	4.815367
305.416608	8000.108332	14.115674	-0.061760	4.815383
305.533704	7999.991612	14.120679	-0.061781	4.815348
305.499281	8000.020968	14.125683	-0.061775	4.815357
305.535590	8000.029050	14.130688	-0.061782	4.815359
305.577082	8000.008355	14.135693	-0.061789	4.815353
305.574523	8000.051068	14.140698	-0.061789	4.815365
305.507437	8000.011465	14.145703	-0.061776	4.815354
305.308727	8000.062680	14.150707	-0.061739	4.815370
305.363093	8000.128788	14.155712	-0.061749	4.815389
305.322237	8000.005169	14.160717	-0.061742	4.815353
305.553125	8000.034656	14.165722	-0.061785	4.815360
305.564120	8000.036972	14.170727	-0.061787	4.815361
305.639998	8000.042504	14.175731	-0.061801	4.815362
305.627685	8000.079711	14.180736	-0.061798	4.815373
305.562051	7999.999509	14.185741	-0.061786	4.815350
305.718499	8000.114351	14.190746	-0.061815	4.815383
305.506971	8000.077693	14.195751	-0.061776	4.815373
305.544373	8000.035549	14.200755	-0.061783	4.815361
305.717747	8000.127154	14.205760	-0.061815	4.815387
305.590386	8000.040581	14.210765	-0.061791	4.815362
305.500688	8000.106434	14.215770	-0.061774	4.815382
305.503454	8000.102200	14.220775	-0.061775	4.815380
305.457524	8000.066155	14.225779	-0.061766	4.815370
305.539969	8000.148766	14.230784	-0.061782	4.815394
305.370109	8000.026210	14.235789	-0.061750	4.815359
305.528746	8000.061980	14.240794	-0.061779	4.815369
305.494567	8000.051787	14.245799	-0.061773	4.815366
305.532859	7999.134159	14.250803	-0.061779	4.815098
305.529317	7996.006628	14.255808	-0.061777	4.814184
305.407358	7990.604037	14.260813	-0.061750	4.812606
305.212908	7983.921543	14.265818	-0.061710	4.810654
304.999108	7976.659731	14.270823	-0.061665	4.808532
305.162116	7968.979319	14.275827	-0.061690	4.806284
305.087408	7961.229401	14.280832	-0.061671	4.804016
304.965011	7953.339602	14.285837	-0.061644	4.801707
305.068794	7945.327126	14.290842	-0.061658	4.799359
305.107402	7937.462387	14.295847	-0.061660	4.797054
304.968473	7929.378444	14.300851	-0.061628	4.794684
305.325694	7921.434587	14.305856	-0.061690	4.792352
305.157178	7913.330524	14.310861	-0.061653	4.789974
305.018386	7905.454180	14.315866	-0.061622	4.787661
304.840471	7897.355940	14.320871	-0.061583	4.785282
305.042092	7889.459272	14.325875	-0.061616	4.782960
305.242689	7881.391249	14.330880	-0.061648	4.780587
304.964628	7873.409784	14.335885	-0.061591	4.778239
305.211845	7865.420285	14.340890	-0.061632	4.775886
305.082519	7857.361864	14.345895	-0.061602	4.773513
304.848979	7849.332636	14.350899	-0.061553	4.771148
304.691842	7841.413268	14.355904	-0.061519	4.768814
304.720878	7833.401783	14.360909	-0.061519	4.766450
304.726346	7825.342156	14.365914	-0.061515	4.764072
304.800908	7817.437505	14.370919	-0.061524	4.761737
304.837255	7809.328114	14.375923	-0.061525	4.759341
304.644120	7801.409118	14.380928	-0.061484	4.757001
304.366371	7793.308412	14.385933	-0.061427	4.754607
304.531875	7785.319287	14.390938	-0.061452	4.752243
304.516073	7777.296201	14.395943	-0.061444	4.749868
304.490298	7769.323403	14.400947	-0.061434	4.747507
304.597650	7761.331804	14.405952	-0.061449	4.745138
304.629635	7753.315988	14.410957	-0.061449	4.742762
304.541716	7745.306091	14.415962	-0.061428	4.740386
304.371536	7737.333065	14.420967	-0.061391	4.738021
304.387513	7729.310251	14.425971	-0.061389	4.735639
304.578958	7721.379365	14.430976	-0.061419	4.733282
304.180575	7713.246076	14.435981	-0.061340	4.730866
304.251199	7705.298937	14.440986	-0.061347	4.728503
304.380849	7697.283911	14.445991	-0.061366	4.726118
304.309935	7689.273165	14.450995	-0.061348	4.723733
304.301604	7681.361381	14.456000	-0.061341	4.721377
304.347327	7673.297947	14.461005	-0.061344	4.718975
304.313570	7665.337399	14.466010	-0.061333	4.716602
304.140027	7657.359833	14.471015	-0.061295	4.714223
303.946391	7649.247099	14.476019	-0.061254	4.711802
304.178309	7641.279979	14.481024	-0.061292	4.709423
304.001787	7633.300066	14.486029	-0.061254	4.707039
304.286401	7625.247332	14.491034	-0.061301	4.704632
304.046358	7617.272008	14.496039	-0.061251	4.702248
304.059284	7609.259864	14.501043	-0.061249	4.699851
304.191761	7601.365260	14.506048	-0.061268	4.697487
303.988951	7593.276383	14.511053	-0.061225	4.695065
303.933444	7585.287526	14.516058	-0.061209	4.692672
303.712879	7577.241338	14.521063	-0.061163	4.690260
303.899823	7569.271619	14.526067	-0.061193	4.687869
303.932529	7561.289380	14.531072	-0.061193	4.685474
303.696228	7553.293027	14.536077	-0.061144	4.683073
303.735030	7545.268128	14.541082	-0.061146	4.680662
303.704047	7537.331095	14.546087	-0.061135	4.678277
303.663845	7529.303632	14.551091	-0.061122	4.675863
303.607454	7521.193118	14.556096	-0.061106	4.673423
303.604977	7513.113051	14.561101	-0.061101	4.670990
303.545883	7505.198602	14.566106	-0.061084	4.668607
303.405682	7497.163576	14.571111	-0.061053	4.666186
303.350361	7489.189044	14.576115	-0.061038	4.663781
303.487280	7481.245300	14.581120	-0.061058	4.661385
303.475429	7473.238838	14.586125	-0.061050	4.658968
303.436582	7465.258149	14.591130	-0.061038	4.656559
303.664851	7457.255682	14.596135	-0.061075	4.654141
303.500287	7449.182698	14.601139	-0.061039	4.651700
303.458089	7441.193863	14.606144	-0.061026	4.649284
303.389692	7433.205004	14.611149	-0.061008	4.646867
303.404850	7425.191696	14.616154	-0.061006	4.644441
303.272293	7417.285247	14.621159	-0.060976	4.642046
303.259076	7409.175186	14.626163	-0.060968	4.639588
303.356013	7401.307435	14.631168	-0.060981	4.637202
303.213192	7393.144904	14.636173	-0.060949	4.634726
303.221635	7385.193730	14.641178	-0.060945	4.632312
303.295239	7377.158425	14.646183	-0.060954	4.629872
303.112812	7369.158836	14.651187	-0.060914	4.627441
303.121595	7361.155535	14.656192	-0.060911	4.625008
303.031820	7353.189191	14.661197	-0.060889	4.622584
303.131660	7345.188242	14.666202	-0.060902	4.620149
303.014832	7337.189309	14.671207	-0.060875	4.617713
302.947349	7329.141400	14.676211	-0.060857	4.615261
302.852873	7321.178683	14.681216	-0.060834	4.612834
302.816319	7313.134242	14.686221	-0.060822	4.610380
302.810850	7305.205583	14.691226	-0.060816	4.607961
302.877283	7297.130800	14.696231	-0.060823	4.605495
302.756710	7289.168735	14.701235	-0.060795	4.603063
302.664962	7281.175171	14.706240	-0.060773	4.600620
302.657983	7273.183773	14.711245	-0.060767	4.598176
302.884854	7265.184117	14.716250	-0.060804	4.595728
302.664720	7257.104639	14.721255	-0.060757	4.593255
302.562460	7249.097693	14.726259	-0.060733	4.590802
302.604791	7241.105003	14.731264	-0.060736	4.588352
302.517460	7233.106649	14.736269	-0.060714	4.585900
302.596545	7225.167193	14.741274	-0.060724	4.583464
302.559913	7217.122395	14.746279	-0.060711	4.580995
302.636243	7209.086751	14.751283	-0.060720	4.578527
302.566801	7201.157386	14.756288	-0.060702	4.576090
302.403063	7193.117846	14.761293	-0.060666	4.573618
302.424675	7185.079102	14.766298	-0.060665	4.571145
302.316022	7177.132347	14.771303	-0.060640	4.568699
302.109492	7169.103082	14.776307	-0.060596	4.566226
302.435988	7161.150226	14.781312	-0.060651	4.563776
302.322614	7153.077701	14.786317	-0.060625	4.561287
302.401212	7145.142411	14.791322	-0.060634	4.558839
302.150575	7137.155127	14.796327	-0.060583	4.556374
301.982523	7129.098119	14.801331	-0.060546	4.553886
301.860733	7121.132248	14.806336	-0.060518	4.551424
301.906704	7113.080069	14.811341	-0.060521	4.548935
302.222105	7105.108624	14.816346	-0.060575	4.546470
302.205755	7097.092704	14.821351	-0.060566	4.543989
301.853127	7089.098127	14.826355	-0.060496	4.541513
302.150315	7081.105399	14.831360	-0.060546	4.539037
301.923371	7073.145154	14.836365	-0.060498	4.536569
301.863804	7065.103797	14.841370	-0.060482	4.534075
301.769448	7057.046998	14.846375	-0.060459	4.531575
301.999127	7049.030810	14.851379	-0.060496	4.529086
302.076706	7041.087264	14.856384	-0.060506	4.526619
301.587674	7033.089628	14.861389	-0.060409	4.524132
301.659342	7025.135818	14.866394	-0.060417	4.521658
301.630852	7017.092780	14.871399	-0.060407	4.519155
301.618292	7009.139307	14.876403	-0.060399	4.516679
301.812859	7001.072420	14.881408	-0.060430	4.514166
301.669709	6993.011581	14.886413	-0.060398	4.511653
301.576090	6985.005942	14.891418	-0.060376	4.509156
301.440216	6977.022130	14.896423	-0.060345	4.506665
301.390005	6969.032084	14.901427	-0.060330	4.504170
301.376245	6961.092140	14.906432	-0.060323	4.501689
301.366427	6953.028737	14.911437	-0.060315	4.499169
301.504982	6945.074326	14.916442	-0.060336	4.496682
301.545178	6937.025424	14.921447	-0.060338	4.494163
301.374557	6929.028848	14.926451	-0.060301	4.491659
301.341081	6921.040483	14.931456	-0.060290	4.489156
301.231687	6913.013519	14.936461	-0.060264	4.486640
301.062103	6905.042460	14.941466	-0.060227	4.484140
301.055160	6897.108098	14.946471	-0.060221	4.481650
301.112645	6889.037327	14.951475	-0.060226	4.479116
301.121506	6881.078919	14.956480	-0.060223	4.476616
300.935241	6873.000940	14.961485	-0.060183	4.474076
301.090611	6864.995367	14.966490	-0.060206	4.471559
301.113963	6857.013563	14.971495	-0.060205	4.469047
301.012034	6849.001970	14.976499	-0.060181	4.466524
301.166123	6840.988057	14.981504	-0.060204	4.464000
301.061761	6833.005398	14.986509	-0.060180	4.461484
300.903401	6825.068506	14.991514	-0.060145	4.458980
300.930232	6817.013252	14.996519	-0.060145	4.456438
301.074446	6808.969064	15.001523	-0.060166	4.453898
300.945440	6800.976276	15.006528	-0.060137	4.451373
300.726280	6793.022791	15.011533	-0.060091	4.448858
300.879519	6784.997094	15.016538	-0.060114	4.446320
300.774586	6777.012815	15.021543	-0.060089	4.443792
300.780907	6768.994205	15.026547	-0.060085	4.441253
300.841079	6761.031675	15.031552	-0.060091	4.438731
300.889807	6752.985204	15.036557	-0.060095	4.436180
300.692278	6744.974294	15.041562	-0.060053	4.433638
300.530606	6736.928228	15.046567	-0.060018	4.431084
300.431764	6728.925297	15.051571	-0.059994	4.428542
300.540588	6720.962334	15.056576	-0.060009	4.426012
300.404093	6712.998623	15.061581	-0.059978	4.423479
300.380320	6704.970177	15.066586	-0.059969	4.420925
300.446537	6697.001915	15.071591	-0.059976	4.418389
300.476676	6688.944677	15.076595	-0.059976	4.415823
300.389491	6680.949744	15.081600	-0.059955	4.413275
300.293599	6672.904791	15.086605	-0.059931	4.410710
300.339691	6664.945487	15.091610	-0.059935	4.408170
300.267334	6656.950602	15.096615	-0.059916	4.405618
300.252584	6648.956529	15.101619	-0.059908	4.403064
300.327848	6640.978335	15.106624	-0.059917	4.400515
300.233461	6633.012420	15.111629	-0.059894	4.397967
300.204442	6624.963264	15.116634	-0.059883	4.395391
300.417154	6616.959609	15.121639	-0.059918	4.392830
300.159345	6608.917915	15.126643	-0.059864	4.390253
300.208614	6601.001362	15.131648	-0.059868	4.387715
300.133546	6592.920274	15.136653	-0.059849	4.385123
299.904903	6585.018857	15.141658	-0.059801	4.382586
299.979081	6576.976742	15.146663	-0.059810	4.380004
300.057818	6569.009209	15.151667	-0.059819	4.377445
300.123627	6560.940724	15.156672	-0.059826	4.374851
299.793257	6552.911474	15.161677	-0.059759	4.372267
299.764438	6544.902830	15.166682	-0.059749	4.369689
299.912569	6536.981855	15.171687	-0.059771	4.367139
299.992561	6528.925341	15.176691	-0.059781	4.364543
299.750921	6521.017225	15.181696	-0.059730	4.361992
299.604645	6512.973650	15.186701	-0.059698	4.359396
299.838899	6505.042534	15.191706	-0.059736	4.356837
299.635978	6496.947811	15.196711	-0.059693	4.354221
299.509402	6488.837206	15.201715	-0.059664	4.351599
299.648703	6480.894111	15.206720	-0.059685	4.349031
299.457068	6472.950825	15.211725	-0.059644	4.346460
299.420599	6464.919487	15.216730	-0.059632	4.343859
299.465422	6456.955840	15.221735	-0.059635	4.341279
299.277577	6448.940171	15.226739	-0.059595	4.338680
299.447475	6440.930488	15.231744	-0.059621	4.336083
299.408654	6432.897300	15.236749	-0.059609	4.333475
299.433348	6424.921423	15.241754	-0.059608	4.330885
299.159622	6416.928942	15.246759	-0.059552	4.328286
299.112247	6408.892265	15.251763	-0.059538	4.325673
299.377893	6400.966752	15.256768	-0.059582	4.323096
299.362398	6392.923662	15.261773	-0.059574	4.320478
299.312299	6384.946606	15.266778	-0.059559	4.317879
299.104322	6376.978919	15.271783	-0.059515	4.315281
299.174279	6368.885353	15.276787	-0.059523	4.312642
299.064134	6360.915647	15.281792	-0.059497	4.310040
298.957525	6352.923960	15.286797	-0.059472	4.307430
298.951975	6344.861242	15.291802	-0.059466	4.304795
298.804323	6336.941440	15.296807	-0.059433	4.302205
298.797402	6328.888591	15.301811	-0.059427	4.299571
298.958052	6320.938685	15.306816	-0.059451	4.296970
298.788169	6312.911019	15.311821	-0.059414	4.294339
298.633926	6304.875586	15.316826	-0.059380	4.291704
298.815606	6296.860679	15.321831	-0.059409	4.289078
299.044539	6288.877979	15.326835	-0.059446	4.286460
298.829787	6280.914971	15.331840	-0.059401	4.283844
298.771337	6272.891232	15.336845	-0.059385	4.281207
298.901316	6264.917051	15.341850	-0.059404	4.278587
298.827762	6256.919711	15.346855	-0.059385	4.275956
298.463634	6248.887411	15.351859	-0.059312	4.273309
298.592393	6240.879658	15.356864	-0.059330	4.270673
298.546991	6232.848217	15.361869	-0.059317	4.268026
298.550160	6224.831861	15.366874	-0.059312	4.265382
298.476773	6216.906700	15.371879	-0.059293	4.262767
298.257861	6208.837194	15.376883	-0.059247	4.260100
298.338598	6200.912136	15.381888	-0.059257	4.257483
298.184600	6192.844406	15.386893	-0.059223	4.254815
298.322191	6184.836109	15.391898	-0.059243	4.252167
298.182935	6176.867720	15.396903	-0.059212	4.249528
298.326367	6168.852216	15.401907	-0.059234	4.246875
298.452979	6160.874162	15.406912	-0.059252	4.244232
298.236228	6152.921038	15.411917	-0.059206	4.241593
298.261150	6144.902159	15.416922	-0.059206	4.238932
298.330874	6136.957537	15.421927	-0.059213	4.236295
298.304536	6128.875928	15.426931	-0.059203	4.233610
298.146890	6120.877423	15.431936	-0.059169	4.230949
297.949394	6112.857034	15.436941	-0.059127	4.228279
298.310479	6104.842326	15.441946	-0.059188	4.225615
298.218212	6096.906799	15.446951	-0.059166	4.222971
298.074522	6088.910388	15.451955	-0.059134	4.220304
297.888234	6080.958738	15.456960	-0.059094	4.217651
298.040574	6072.875743	15.461965	-0.059117	4.214955
297.747789	6064.887033	15.466970	-0.059057	4.212284
297.771226	6056.888288	15.471975	-0.059057	4.209612
297.955871	6048.909285	15.476979	-0.059086	4.206946
297.895511	6040.892450	15.481984	-0.059069	4.204263
297.608175	6032.940942	15.486989	-0.059010	4.201598
297.481313	6024.927174	15.491994	-0.058982	4.198912
297.605093	6016.927482	15.496999	-0.058999	4.196232
297.531964	6008.823701	15.502003	-0.058980	4.193513
297.561459	6000.815867	15.507008	-0.058981	4.190826
297.548336	5992.835903	15.512013	-0.058973	4.188145
297.331408	5984.850902	15.517018	-0.058927	4.185460
297.493314	5976.908975	15.522023	-0.058952	4.182791
297.592502	5968.839617	15.527027	-0.058965	4.180076
297.577741	5960.931209	15.532032	-0.058957	4.177413
297.344750	5952.864610	15.537037	-0.058909	4.174693
297.346132	5944.865031	15.542042	-0.058904	4.171996
297.367221	5936.863500	15.547047	-0.058902	4.169296
297.334795	5928.859699	15.552051	-0.058891	4.166594
297.341962	5920.898580	15.557056	-0.058887	4.163905
297.380472	5912.889842	15.562061	-0.058889	4.161198
297.354213	5904.875598	15.567066	-0.058879	4.158487
297.174320	5896.878325	15.572071	-0.058840	4.155778
297.142346	5888.842543	15.577075	-0.058829	4.153056
297.300226	5880.845982	15.582080	-0.058853	4.150347
297.190278	5872.857485	15.587085	-0.058827	4.147637
296.929894	5864.810566	15.592090	-0.058774	4.144903
297.162266	5856.885871	15.597095	-0.058812	4.142215
296.913180	5848.851970	15.602099	-0.058760	4.139482
296.895879	5840.890482	15.607104	-0.058751	4.136774
296.909133	5832.867085	15.612109	-0.058749	4.134044
296.868318	5824.805107	15.617114	-0.058736	4.131299
296.801242	5816.835570	15.622119	-0.058718	4.128583
296.785919	5808.855697	15.627123	-0.058710	4.125862
296.802698	5800.895476	15.632128	-0.058708	4.123146
296.577461	5792.851593	15.637133	-0.058661	4.120397
296.601574	5784.884344	15.642138	-0.058660	4.117676
296.671068	5776.863154	15.647143	-0.058667	4.114935
296.448218	5768.796181	15.652147	-0.058621	4.112172
296.488197	5760.824228	15.657152	-0.058623	4.109444
296.564801	5752.815174	15.662157	-0.058632	4.106702
296.550488	5744.845858	15.667162	-0.058624	4.103970
296.330902	5736.864220	15.672167	-0.058578	4.101229
296.408438	5728.828421	15.677171	-0.058587	4.098472
296.622598	5720.859979	15.682176	-0.058622	4.095738
296.489766	5712.867546	15.687181	-0.058592	4.092990
296.523122	5704.856828	15.692186	-0.058593	4.090235
296.556882	5696.880505	15.697191	-0.058594	4.087491
296.407391	5688.819771	15.702195	-0.058560	4.084713
296.386604	5680.918896	15.707200	-0.058551	4.081990
296.359907	5672.895028	15.712205	-0.058541	4.079222
296.175577	5664.922711	15.717210	-0.058502	4.076469
296.046744	5656.895795	15.722215	-0.058472	4.073695
296.242274	5648.823399	15.727219	-0.058503	4.070909
296.418388	5640.879089	15.732224	-0.058531	4.068164
296.129137	5632.853484	15.737229	-0.058472	4.065383
296.062779	5624.910913	15.742234	-0.058454	4.062632
296.227111	5616.882314	15.747239	-0.058480	4.059852
296.150466	5608.922205	15.752243	-0.058460	4.057091
296.013750	5600.916975	15.757248	-0.058429	4.054312
296.033644	5592.890100	15.762253	-0.058428	4.051525
296.145538	5584.865795	15.767258	-0.058443	4.048739
296.066257	5576.917848	15.772263	-0.058423	4.045974
295.788649	5568.919166	15.777267	-0.058366	4.043187
295.869598	5560.903735	15.782272	-0.058376	4.040398
295.898124	5552.948003	15.787277	-0.058376	4.037626
295.846912	5544.884773	15.792282	-0.058361	4.034814
295.921441	5536.794949	15.797287	-0.058370	4.031993
295.657859	5528.815658	15.802291	-0.058316	4.029203
295.628675	5520.858634	15.807296	-0.058305	4.026423
295.438706	5512.865933	15.812301	-0.058264	4.023625
295.725106	5504.879425	15.817306	-0.058312	4.020835
295.440412	5496.921684	15.822311	-0.058254	4.018045
295.310424	5488.857650	15.827315	-0.058225	4.015218
295.644297	5480.885593	15.832320	-0.058282	4.012428
295.462813	5472.841399	15.837325	-0.058243	4.009603
295.302395	5464.871349	15.842330	-0.058207	4.006802
295.545894	5456.836380	15.847335	-0.058247	4.003983
295.473774	5448.870934	15.852339	-0.058229	4.001181
295.569198	5440.948747	15.857344	-0.058241	3.998395
295.248992	5432.912692	15.862349	-0.058176	3.995561
295.202137	5424.862010	15.867354	-0.058162	3.992724
295.312571	5416.865619	15.872359	-0.058178	3.989906
295.129469	5408.879529	15.877363	-0.058138	3.987085
295.273620	5400.853083	15.882368	-0.058160	3.984254
295.201625	5392.867073	15.887373	-0.058141	3.981431
295.030072	5384.874643	15.892378	-0.058104	3.978602
294.944130	5376.921007	15.897383	-0.058083	3.975786
294.804773	5368.891832	15.902387	-0.058052	3.972941
294.829105	5360.884517	15.907392	-0.058051	3.970104
294.758614	5352.895345	15.912397	-0.058032	3.967270
294.951813	5344.882640	15.917402	-0.058063	3.964430
294.923401	5336.952123	15.922407	-0.058053	3.961613
294.688094	5328.933575	15.927411	-0.058004	3.958759
294.860514	5320.944247	15.932416	-0.058030	3.955921
294.814310	5312.894882	15.937421	-0.058017	3.953056
294.579471	5304.885090	15.942426	-0.057968	3.950199
294.699995	5296.902378	15.947431	-0.057985	3.947356
294.811182	5288.862827	15.952435	-0.058000	3.944491
294.751380	5280.933678	15.957440	-0.057984	3.941660
294.600101	5272.957108	15.962445	-0.057950	3.938808
294.652375	5264.945729	15.967450	-0.057955	3.935946
294.674877	5256.937284	15.972455	-0.057954	3.933082
294.643549	5248.866738	15.977459	-0.057943	3.930192
294.442265	5240.940490	15.982464	-0.057900	3.927349
294.501120	5232.942545	15.987469	-0.057906	3.924483
294.502505	5224.956811	15.992474	-0.057901	3.921618
294.507107	5216.957630	15.997479	-0.057896	3.918747
294.428683	5208.952043	16.002483	-0.057876	3.915869
294.422574	5200.944342	16.007488	-0.057870	3.912990
294.382047	5192.912217	16.012493	-0.057857	3.910100
294.231895	5184.950646	16.017498	-0.057824	3.907230
294.411871	5176.965791	16.022503	-0.057852	3.904356
294.203886	5168.970539	16.027507	-0.057808	3.901469
294.087341	5160.973076	16.032512	-0.057781	3.898581
294.138211	5152.943456	16.037517	-0.057785	3.895682
294.079619	5144.967859	16.042522	-0.057769	3.892799
294.063265	5136.915727	16.047527	-0.057761	3.889886
294.130191	5128.916971	16.052531	-0.057768	3.886993
293.934115	5120.947589	16.057536	-0.057726	3.884102
293.720133	5112.981739	16.062541	-0.057681	3.881211
293.899263	5104.938961	16.067546	-0.057709	3.878297
293.967134	5096.992377	16.072551	-0.057717	3.875413
293.714528	5088.766569	16.077555	-0.057664	3.872420
293.731966	5080.790148	16.082560	-0.057662	3.869520
293.770524	5072.850295	16.087565	-0.057664	3.866632
293.818122	5064.872161	16.092570	-0.057668	3.863728
293.760907	5056.937427	16.097575	-0.057652	3.860835
293.534403	5048.918681	16.102579	-0.057605	3.857907
293.547423	5040.932285	16.107584	-0.057602	3.854992
293.544817	5032.941685	16.112589	-0.057596	3.852074
293.467928	5024.909180	16.117594	-0.057576	3.849136
293.510792	5016.951268	16.122599	-0.057579	3.846226
293.312880	5008.959944	16.127603	-0.057537	3.843297
293.402725	5000.985103	16.132608	-0.057549	3.840377
293.559790	4992.974212	16.137613	-0.057573	3.837443
293.282790	4985.004064	16.142618	-0.057516	3.834513
293.311609	4976.987137	16.147623	-0.057516	3.831570
293.284193	4968.959174	16.152627	-0.057505	3.828620
293.296082	4960.988642	16.157632	-0.057502	3.825689
293.119398	4953.047716	16.162637	-0.057464	3.822762
293.233922	4944.990341	16.167642	-0.057480	3.819797
293.446948	4937.031725	16.172647	-0.057515	3.816868
293.382155	4929.001265	16.177651	-0.057497	3.813904
293.382900	4921.018933	16.182656	-0.057492	3.810958
293.058118	4913.062544	16.187661	-0.057427	3.808011
293.088028	4905.018350	16.192666	-0.057427	3.805037
293.120117	4897.107658	16.197671	-0.057428	3.802111
293.127960	4889.028346	16.202675	-0.057424	3.799119
293.120676	4881.086810	16.207680	-0.057417	3.796175
293.034065	4873.040017	16.212685	-0.057396	3.793189
292.994743	4865.007732	16.217690	-0.057383	3.790206
292.994204	4857.010569	16.222695	-0.057378	3.787236
292.806905	4849.018240	16.227699	-0.057338	3.784260
292.803240	4841.083360	16.232704	-0.057332	3.781308
292.826018	4833.055880	16.237709	-0.057331	3.778319
292.827456	4825.017611	16.242714	-0.057326	3.775323
292.790586	4817.055820	16.247719	-0.057314	3.772353
292.577583	4808.997293	16.252723	-0.057269	3.769340
292.742986	4801.044263	16.257728	-0.057294	3.766373
292.373937	4793.063265	16.262733	-0.057220	3.763381
292.322156	4785.065191	16.267738	-0.057205	3.760387
292.564926	4777.096267	16.272743	-0.057245	3.757409
292.469871	4769.029456	16.277747	-0.057222	3.754384
292.382328	4761.069415	16.282752	-0.057201	3.751396
292.336426	4753.045832	16.287757	-0.057187	3.748384
292.556843	4745.011337	16.292762	-0.057223	3.745370
292.405819	4737.096864	16.297767	-0.057189	3.742391
292.390197	4729.045098	16.302771	-0.057181	3.739362
292.347359	4721.126720	16.307776	-0.057168	3.736379
292.317369	4713.078076	16.312781	-0.057157	3.733345
292.191472	4705.027985	16.317786	-0.057128	3.730306
292.268783	4697.108882	16.322791	-0.057138	3.727318
292.136076	4689.058274	16.327795	-0.057108	3.724274
292.081209	4681.171129	16.332800	-0.057092	3.721290
292.011609	4673.151903	16.337805	-0.057074	3.718254
292.136835	4665.143254	16.342810	-0.057092	3.715224
292.040115	4657.050794	16.347815	-0.057069	3.712155
292.076735	4649.013242	16.352819	-0.057070	3.709107
292.095437	4641.072223	16.357824	-0.057068	3.706092
291.982031	4633.091205	16.362829	-0.057042	3.703057
291.869961	4625.102748	16.367834	-0.057016	3.700017
291.858868	4617.186482	16.372839	-0.057009	3.697003
291.724931	4609.135606	16.377843	-0.056978	3.693934
291.773898	4601.148244	16.382848	-0.056982	3.690890
291.671089	4593.163545	16.387853	-0.056958	3.687841
291.886261	4585.108108	16.392858	-0.056993	3.684771
291.797740	4577.202719	16.397863	-0.056971	3.681747
291.590154	4569.160832	16.402867	-0.056927	3.678666
291.603014	4561.190172	16.407872	-0.056924	3.675615
291.464041	4553.178441	16.412877	-0.056893	3.672542
291.411291	4545.157940	16.417882	-0.056878	3.669466
291.557667	4537.214571	16.422887	-0.056900	3.666421
291.533531	4529.162482	16.427891	-0.056890	3.663328
291.437478	4521.186206	16.432896	-0.056867	3.660259
291.447161	4513.224911	16.437901	-0.056864	3.657196
291.188845	4505.178285	16.442906	-0.056810	3.654091
291.339423	4497.179573	16.447911	-0.056833	3.651013
291.243062	4489.193911	16.452915	-0.056810	3.647930
291.335535	4481.179467	16.457920	-0.056822	3.644839
291.276608	4473.239544	16.462925	-0.056806	3.641769
291.063178	4465.205630	16.467930	-0.056760	3.638657
291.185932	4457.274785	16.472935	-0.056778	3.635591
291.041312	4449.207184	16.477939	-0.056746	3.632462
290.956389	4441.202020	16.482944	-0.056725	3.629356
290.973785	4433.215117	16.487949	-0.056723	3.626258
291.047967	4425.209372	16.492954	-0.056731	3.623151
291.101722	4417.223943	16.497959	-0.056736	3.620048
290.857553	4409.259867	16.502963	-0.056685	3.616943
291.096980	4401.243007	16.507968	-0.056725	3.613829
290.845414	4393.251648	16.512973	-0.056673	3.610708
290.614742	4385.256235	16.517978	-0.056624	3.607583
290.737405	4377.253938	16.522983	-0.056642	3.604462
290.823402	4369.293083	16.527987	-0.056653	3.601354
290.913435	4361.324415	16.532992	-0.056664	3.598241
290.663981	4353.335906	16.537997	-0.056613	3.595107
290.613286	4345.282044	16.543002	-0.056598	3.591951
290.540761	4337.327600	16.548007	-0.056579	3.588830
290.386498	4329.305698	16.553011	-0.056545	3.585678
290.818989	4321.323910	16.558016	-0.056620	3.582555
290.730474	4313.312107	16.563021	-0.056599	3.579403
290.553281	4305.336864	16.568026	-0.056560	3.576260
290.657164	4297.348198	16.573031	-0.056574	3.573117
290.580584	4289.332224	16.578035	-0.056555	3.569956
290.528587	4281.380916	16.583040	-0.056540	3.566818
290.339518	4273.377962	16.588045	-0.056500	3.563652
290.419043	4265.342651	16.593050	-0.056509	3.560479
290.492193	4257.407252	16.598055	-0.056517	3.557342
290.236405	4249.349513	16.603059	-0.056465	3.554145
290.172815	4241.282494	16.608064	-0.056447	3.550946
290.239443	4233.309060	16.613069	-0.056455	3.547786
290.257339	4225.314118	16.618074	-0.056453	3.544613
290.187413	4217.380825	16.623079	-0.056434	3.541458
290.121068	4209.367265	16.628083	-0.056417	3.538270
290.197887	4201.386245	16.633088	-0.056426	3.535095
289.979535	4193.366510	16.638093	-0.056380	3.531894
289.935096	4185.381678	16.643098	-0.056366	3.528708
290.259495	4177.376866	16.648103	-0.056422	3.525523
290.015107	4169.400559	16.653107	-0.056371	3.522329
289.981438	4161.422550	16.658112	-0.056359	3.519138
289.800895	4153.453675	16.663117	-0.056320	3.515944
289.760754	4145.423718	16.668122	-0.056308	3.512726
289.887766	4137.406193	16.673127	-0.056326	3.509515
289.898172	4129.395608	16.678131	-0.056323	3.506301
289.791516	4121.462011	16.683136	-0.056298	3.503111
289.700620	4113.456857	16.688141	-0.056275	3.499889
289.653142	4105.472033	16.693146	-0.056261	3.496675
289.937863	4097.448577	16.698151	-0.056309	3.493452
289.694816	4089.433336	16.703155	-0.056259	3.490213
289.552983	4081.512850	16.708160	-0.056227	3.487012
289.766285	4073.489962	16.713165	-0.056261	3.483778
289.510164	4065.549928	16.718170	-0.056208	3.480560
289.711353	4057.559728	16.723175	-0.056241	3.477333
289.414640	4049.532986	16.728179	-0.056180	3.474072
289.351339	4041.533152	16.733184	-0.056163	3.470827
289.289764	4033.541467	16.738189	-0.056146	3.467582
289.324883	4025.521176	16.743194	-0.056148	3.464326
289.345757	4017.588608	16.748199	-0.056146	3.461101
289.153810	4009.547020	16.753203	-0.056105	3.457822
289.089156	4001.574196	16.758208	-0.056088	3.454573
289.074126	3993.562825	16.763213	-0.056080	3.451306
289.039635	3985.572855	16.768218	-0.056068	3.448044
289.054866	3977.575756	16.773223	-0.056066	3.444778
289.142728	3969.598679	16.778227	-0.056077	3.441519
289.098600	3961.622293	16.783232	-0.056063	3.438253
288.873189	3953.613409	16.788237	-0.056016	3.434965
288.810347	3945.586876	16.793242	-0.055999	3.431671
288.905244	3937.583324	16.798247	-0.056012	3.428389
288.648187	3929.581284	16.803251	-0.055958	3.425093
288.724351	3921.660637	16.808256	-0.055967	3.421839
288.798575	3913.620296	16.813261	-0.055976	3.418531
288.840401	3905.629761	16.818266	-0.055979	3.415241
288.688363	3897.653105	16.823271	-0.055945	3.411946
288.705923	3889.627091	16.828275	-0.055943	3.408633
288.672077	3881.647127	16.833280	-0.055931	3.405334
288.517975	3873.721141	16.838285	-0.055897	3.402050
288.673278	3865.704710	16.843290	-0.055921	3.398737
288.621335	3857.745741	16.848295	-0.055906	3.395436
288.429387	3849.659596	16.853299	-0.055865	3.392075
288.461867	3841.644611	16.858304	-0.055866	3.388748
288.481044	3833.673141	16.863309	-0.055864	3.385435
288.341447	3825.712372	16.868314	-0.055833	3.382118
288.354806	3817.741298	16.873319	-0.055830	3.378799
288.345671	3809.737297	16.878323	-0.055823	3.375462
288.403766	3801.731768	16.883328	-0.055829	3.372123
288.420677	3793.733917	16.888333	-0.055827	3.368783
288.293478	3785.748838	16.893338	-0.055798	3.365440
288.228203	3777.803735	16.898343	-0.055780	3.362112
288.116413	3769.802747	16.903347	-0.055754	3.358756
288.015148	3761.826022	16.908352	-0.055730	3.355407
287.915032	3753.812616	16.913357	-0.055706	3.352039
288.057729	3745.775210	16.918362	-0.055728	3.348667
288.115154	3737.781406	16.923367	-0.055733	3.345306
287.926585	3729.837698	16.928371	-0.055693	3.341954
288.185505	3721.850568	16.933376	-0.055736	3.338597
287.826827	3713.870431	16.938381	-0.055664	3.335217
287.795064	3705.849328	16.943386	-0.055652	3.331828
287.890301	3697.853339	16.948391	-0.055665	3.328451
287.826929	3689.851316	16.953395	-0.055648	3.325062
287.890871	3681.919215	16.958400	-0.055655	3.321704
287.792854	3673.920342	16.963405	-0.055631	3.318308
287.893674	3665.908480	16.968410	-0.055645	3.314911
287.655580	3657.900260	16.973415	-0.055595	3.311499
287.428139	3649.902402	16.978419	-0.055547	3.308088
287.494244	3641.913934	16.983424	-0.055554	3.304689
287.431270	3633.962721	16.988429	-0.055537	3.301297
287.411889	3625.966828	16.993434	-0.055529	3.297884
287.471688	3617.968492	16.998439	-0.055534	3.294470
287.215790	3609.972421	17.003443	-0.055482	3.291041
287.479903	3601.976006	17.008448	-0.055525	3.287629
287.367067	3594.004228	17.013453	-0.055499	3.284209
287.424496	3586.009447	17.018458	-0.055505	3.280781
287.520983	3578.045628	17.023463	-0.055517	3.277366
287.244310	3570.041843	17.028467	-0.055461	3.273915
287.254979	3562.008220	17.033472	-0.055457	3.270458
287.225281	3554.041092	17.038477	-0.055446	3.267025
287.042363	3546.047118	17.043482	-0.055407	3.263571
287.307385	3538.060530	17.048487	-0.055451	3.260134
287.213188	3530.092746	17.053491	-0.055428	3.256687
287.132766	3522.081688	17.058496	-0.055408	3.253219
287.269072	3514.073700	17.063501	-0.055428	3.249757
287.164994	3506.107131	17.068506	-0.055404	3.246299
287.041913	3498.150859	17.073511	-0.055376	3.242841
287.007548	3490.139620	17.078515	-0.055364	3.239360
287.003292	3482.216018	17.083520	-0.055358	3.235914
286.829558	3474.143161	17.088525	-0.055320	3.232392
286.826507	3466.092652	17.093530	-0.055314	3.228883
287.000708	3458.103732	17.098535	-0.055342	3.225405
286.864827	3450.151626	17.103539	-0.055311	3.221926
286.801566	3442.199948	17.108544	-0.055294	3.218446
286.675386	3434.215763	17.113549	-0.055265	3.214946
286.669389	3426.213366	17.118554	-0.055259	3.211439
286.769828	3418.213239	17.123559	-0.055272	3.207934
286.498674	3410.212152	17.128563	-0.055217	3.204409
286.567429	3402.267320	17.133568	-0.055224	3.200919
286.543749	3394.279629	17.138573	-0.055215	3.197402
286.486020	3386.259363	17.143578	-0.055198	3.193866
286.578522	3378.259170	17.148583	-0.055210	3.190341
286.390480	3370.284657	17.153587	-0.055170	3.186811
286.413188	3362.299627	17.158592	-0.055169	3.183282
286.440187	3354.323739	17.163597	-0.055169	3.179753
286.262019	3346.357378	17.168602	-0.055131	3.176216
286.288238	3338.342334	17.173607	-0.055130	3.172662
286.102316	3330.346171	17.178611	-0.055090	3.169103
286.184360	3322.361979	17.183616	-0.055100	3.165557
286.218242	3314.395565	17.188621	-0.055101	3.162013
285.937101	3306.418196	17.193626	-0.055044	3.158447
285.948440	3298.440447	17.198631	-0.055041	3.154889
285.901330	3290.365595	17.203635	-0.055027	3.151280
286.009131	3282.402850	17.208640	-0.055041	3.147725
285.968622	3274.432876	17.213645	-0.055029	3.144156
285.961438	3266.440161	17.218650	-0.055022	3.140574
285.930146	3258.479107	17.223655	-0.055011	3.137001
285.727046	3250.473173	17.228659	-0.054968	3.133397
285.491534	3242.490852	17.233664	-0.054919	3.129797
285.619553	3234.499970	17.238669	-0.054937	3.126206
285.411162	3226.545946	17.243674	-0.054893	3.122611
285.451364	3218.577933	17.248679	-0.054896	3.119018
285.480298	3210.565637	17.253683	-0.054896	3.115400
285.730160	3202.561356	17.258688	-0.054937	3.111791
285.586676	3194.566166	17.263693	-0.054905	3.108165
285.411452	3186.574605	17.268698	-0.054867	3.104534
285.540139	3178.617759	17.273703	-0.054886	3.100929
285.437278	3170.632890	17.278707	-0.054861	3.097296
285.393504	3162.630245	17.283712	-0.054848	3.093654
285.317919	3154.629290	17.288717	-0.054829	3.090006
285.378830	3146.650061	17.293722	-0.054835	3.086371
285.118618	3138.718801	17.298727	-0.054781	3.082738
285.299132	3130.684828	17.303731	-0.054809	3.079074
285.285167	3122.735964	17.308736	-0.054802	3.075436
285.229719	3114.670652	17.313741	-0.054786	3.071738
285.007853	3106.659233	17.318746	-0.054739	3.068053
285.187538	3098.675026	17.323751	-0.054768	3.064395
285.109460	3090.713034	17.328755	-0.054748	3.060730
285.142442	3082.764159	17.333760	-0.054749	3.057072
285.346186	3074.747696	17.338765	-0.054781	3.053387
285.243360	3066.752707	17.343770	-0.054757	3.049693
285.014895	3058.837798	17.348775	-0.054709	3.046025
284.937225	3050.841441	17.353779	-0.054689	3.042323
285.082476	3042.860118	17.358784	-0.054711	3.038633
285.047134	3034.873472	17.363789	-0.054699	3.034928
284.940459	3026.863006	17.368794	-0.054674	3.031204
284.800381	3018.904842	17.373799	-0.054643	3.027497
284.726675	3010.891264	17.378803	-0.054624	3.023764
284.561161	3002.947415	17.383808	-0.054588	3.020054
284.614074	2994.985238	17.388813	-0.054593	3.016342
284.595796	2986.951462	17.393818	-0.054584	3.012588
284.595063	2978.964559	17.398823	-0.054578	3.008852
284.572557	2970.955889	17.403827	-0.054569	3.005101
284.499509	2963.031090	17.408832	-0.054550	3.001381
284.500783	2955.054485	17.413837	-0.054545	2.997636
284.411340	2947.060930	17.418842	-0.054523	2.993874
284.454021	2939.035641	17.423847	-0.054526	2.990099
284.246031	2931.079493	17.428851	-0.054482	2.986339
284.262796	2923.108272	17.433856	-0.054480	2.982579
284.250119	2915.113249	17.438861	-0.054472	2.978801
284.182821	2907.124968	17.443866	-0.054454	2.975018
284.147374	2899.153361	17.448871	-0.054443	2.971241
284.142660	2891.151124	17.453875	-0.054436	2.967445
284.040768	2883.196486	17.458880	-0.054412	2.963663
284.079840	2875.191641	17.463885	-0.054414	2.959859
283.899098	2867.257418	17.468890	-0.054375	2.956072
283.903842	2859.240162	17.473895	-0.054371	2.952250
283.933773	2851.205074	17.478899	-0.054371	2.948416
284.049056	2843.222760	17.483904	-0.054387	2.944607
283.738426	2835.294914	17.488909	-0.054324	2.940797
283.710078	2827.316261	17.493914	-0.054314	2.936972
283.663195	2819.340930	17.498919	-0.054300	2.933143
283.630924	2811.330289	17.503923	-0.054289	2.929293
283.786764	2803.325233	17.508928	-0.054312	2.925450
283.738281	2795.402825	17.513933	-0.054298	2.921631
283.437789	2787.445310	17.518938	-0.054237	2.917777
283.492332	2779.429156	17.523943	-0.054242	2.913908
283.486532	2771.340581	17.528947	-0.054235	2.909996
283.438574	2763.395734	17.533952	-0.054221	2.906146
283.463111	2755.427067	17.538957	-0.054221	2.902283
283.418388	2747.456087	17.543962	-0.054207	2.898410
283.374182	2739.494446	17.548967	-0.054194	2.894537
283.221656	2731.485007	17.553971	-0.054160	2.890629
283.482471	2723.510326	17.558976	-0.054203	2.886755
283.420910	2715.537342	17.563981	-0.054187	2.882860
283.276261	2707.590174	17.568986	-0.054154	2.878967
283.366727	2699.602726	17.573991	-0.054166	2.875062
283.249994	2691.598973	17.578995	-0.054139	2.871132
283.116946	2683.630950	17.584000	-0.054109	2.867214
282.956037	2675.673845	17.589005	-0.054074	2.863294
283.153785	2667.663951	17.594010	-0.054105	2.859362
283.092940	2659.718142	17.599015	-0.054089	2.855443
282.923806	2651.708259	17.604019	-0.054052	2.851480
283.005724	2643.722895	17.609024	-0.054062	2.847538
282.987344	2635.755486	17.614029	-0.054053	2.843593
282.806422	2627.804982	17.619034	-0.054014	2.839643
282.821724	2619.840210	17.624039	-0.054012	2.835691
282.739470	2611.805985	17.629043	-0.053991	2.831693
282.674234	2603.827597	17.634048	-0.053974	2.827718
282.614162	2595.855491	17.639053	-0.053958	2.823741
282.670799	2587.855049	17.644058	-0.053963	2.819752
282.707652	2579.908114	17.649063	-0.053965	2.815782
282.580911	2571.904498	17.654067	-0.053936	2.811768
282.524995	2563.935358	17.659072	-0.053920	2.807771
282.710005	2555.956699	17.664077	-0.053949	2.803776
282.359831	2548.001992	17.669082	-0.053879	2.799757
282.494324	2540.055595	17.674087	-0.053899	2.795765
282.410048	2532.022634	17.679091	-0.053878	2.791710
282.321415	2524.044533	17.684096	-0.053856	2.787677
282.260904	2516.085868	17.689101	-0.053839	2.783650
282.429278	2508.092422	17.694106	-0.053865	2.779613
282.536118	2500.149657	17.699111	-0.053880	2.775591
282.093191	2492.160835	17.704115	-0.053792	2.771509
282.215629	2484.170108	17.709120	-0.053810	2.767452
282.357617	2476.200379	17.714125	-0.053831	2.763402
282.269876	2468.222091	17.719130	-0.053810	2.759327
282.156645	2460.295884	17.724135	-0.053783	2.755272
282.224444	2452.212532	17.729139	-0.053791	2.751141
282.170639	2444.239033	17.734144	-0.053775	2.747052
281.870607	2436.307098	17.739149	-0.053714	2.742964
281.938348	2428.315148	17.744154	-0.053722	2.738862
281.885258	2420.369443	17.749159	-0.053706	2.734769
281.535885	2412.387873	17.754163	-0.053636	2.730634
281.652695	2404.403706	17.759168	-0.053653	2.726520
281.838398	2396.414275	17.764173	-0.053682	2.722401
281.661715	2388.450488	17.769178	-0.053644	2.718267
281.685677	2380.503844	17.774183	-0.053643	2.714148
281.550887	2372.494518	17.779187	-0.053613	2.709980
281.685599	2364.522895	17.784192	-0.053633	2.705842
281.527081	2356.578795	17.789197	-0.053598	2.701694
281.526694	2348.590318	17.794202	-0.053592	2.697526
281.405240	2340.655618	17.799207	-0.053565	2.693372
281.249883	2332.646707	17.804211	-0.053530	2.689171
281.383380	2324.655406	17.809216	-0.053550	2.684991
281.281969	2316.720322	17.814221	-0.053526	2.680818
281.185088	2308.748449	17.819226	-0.053503	2.676621
281.260694	2300.762291	17.824231	-0.053511	2.672420
281.225855	2292.751790	17.829235	-0.053500	2.668192
281.149515	2284.794482	17.834240	-0.053480	2.663983
281.228953	2276.798969	17.839245	-0.053490	2.659758
281.069414	2268.862354	17.844250	-0.053455	2.655541
281.131614	2260.866662	17.849255	-0.053461	2.651301
281.152953	2252.883446	17.854259	-0.053460	2.647058
281.183911	2244.936731	17.859264	-0.053460	2.642828
281.092880	2236.992552	17.864269	-0.053438	2.638585
280.782548	2229.046725	17.869274	-0.053375	2.634319
280.846490	2221.017695	17.874279	-0.053382	2.630027
280.666800	2213.067008	17.879283	-0.053343	2.625753
280.884828	2205.078756	17.884288	-0.053379	2.621479
280.816297	2197.135974	17.889293	-0.053361	2.617204
280.719738	2189.154375	17.894298	-0.053337	2.612898
280.767683	2181.174690	17.899303	-0.053341	2.608596
280.559803	2173.216865	17.904307	-0.053297	2.604282
280.598712	2165.258893	17.909312	-0.053299	2.599976
280.619019	2157.308628	17.914317	-0.053298	2.595667
280.528473	2149.151067	17.919322	-0.053275	2.591230
280.479584	2141.187510	17.924327	-0.053261	2.586895
280.585608	2133.231078	17.929331	-0.053276	2.582566
280.562976	2125.303211	17.934336	-0.053266	2.578237
280.469959	2117.365286	17.939341	-0.053244	2.573890
280.454712	2109.370944	17.944346	-0.053235	2.569510
280.586676	2101.435635	17.949351	-0.053255	2.565166
280.422180	2093.492951	17.954355	-0.053219	2.560789
280.341233	2085.557054	17.959360	-0.053199	2.556415
280.469533	2077.553410	17.964365	-0.053217	2.552010
280.132904	2069.613456	17.969370	-0.053149	2.547600
280.174369	2061.651241	17.974375	-0.053152	2.543197
279.998754	2053.689336	17.979379	-0.053114	2.538771
280.092118	2045.711908	17.984384	-0.053126	2.534347
279.892772	2037.755991	17.989389	-0.053084	2.529907
279.828655	2029.764684	17.994394	-0.053067	2.525449
279.940525	2021.814438	17.999399	-0.053082	2.521019
279.758580	2013.864453	18.004403	-0.053043	2.516560
279.734699	2005.866887	18.009408	-0.053033	2.512078
279.757207	1997.886529	18.014413	-0.053032	2.507601
279.775979	1989.895921	18.019418	-0.053031	2.503109
279.749057	1981.973711	18.024423	-0.053020	2.498645
279.548771	1974.017032	18.029427	-0.052978	2.494141
279.786423	1966.005768	18.034432	-0.053017	2.489630
279.717877	1958.067273	18.039437	-0.052999	2.485129
279.439140	1950.136659	18.044442	-0.052942	2.480609
279.663490	1942.176140	18.049447	-0.052978	2.476101
279.510398	1934.193642	18.054451	-0.052944	2.471544
279.394883	1926.231171	18.059456	-0.052918	2.466993
279.450550	1918.275849	18.064461	-0.052923	2.462451
279.522643	1910.290527	18.069466	-0.052931	2.457884
279.494960	1902.346106	18.074471	-0.052921	2.453325
279.393295	1894.364023	18.079475	-0.052896	2.448729
279.565462	1886.394609	18.084480	-0.052923	2.444154
279.345607	1878.497501	18.089485	-0.052877	2.439581
279.153968	1870.540108	18.094490	-0.052836	2.434968
279.192334	1862.490283	18.099495	-0.052838	2.430309
279.170342	1854.514366	18.104499	-0.052829	2.425680
279.116272	1846.586630	18.109504	-0.052813	2.421068
279.123892	1838.645773	18.114509	-0.052810	2.416443
278.888651	1830.683368	18.119514	-0.052761	2.411779
278.909164	1822.719070	18.124519	-0.052759	2.407124
278.740176	1814.779926	18.129523	-0.052722	2.402460
278.738522	1806.831613	18.134528	-0.052717	2.397795
278.800824	1798.851777	18.139533	-0.052723	2.393107
278.355000	1790.904606	18.144538	-0.052635	2.388390
278.295927	1782.968948	18.149543	-0.052619	2.383700
278.526869	1774.966314	18.154547	-0.052657	2.378984
278.654170	1767.001189	18.159552	-0.052675	2.374273
278.629209	1759.035220	18.164557	-0.052665	2.369540
278.665496	1751.070119	18.169562	-0.052667	2.364803
278.320637	1743.191403	18.174567	-0.052597	2.360077
278.289999	1735.237991	18.179571	-0.052586	2.355322
278.272063	1727.233556	18.184576	-0.052578	2.350528
278.275841	1719.267727	18.189581	-0.052573	2.345750
278.284121	1711.302981	18.194586	-0.052569	2.340962
278.127256	1703.395566	18.199591	-0.052535	2.336186
278.149709	1695.393758	18.204595	-0.052534	2.331358
278.048014	1687.449890	18.209600	-0.052510	2.326544
278.082509	1679.502925	18.214605	-0.052511	2.321730
278.205046	1671.544218	18.219610	-0.052529	2.316906
278.128469	1663.602310	18.224615	-0.052509	2.312066
277.902265	1655.647703	18.229619	-0.052462	2.307195
278.202090	1647.657826	18.234624	-0.052512	2.302336
278.304919	1639.723354	18.239629	-0.052526	2.297485
278.029512	1631.784389	18.244634	-0.052470	2.292588
277.987538	1623.836258	18.249639	-0.052457	2.287696
278.006211	1615.881357	18.254643	-0.052455	2.282793
277.803266	1607.973101	18.259648	-0.052412	2.277890
277.775990	1599.995002	18.264653	-0.052402	2.272949
277.727745	1591.967300	18.269658	-0.052387	2.267963
277.576199	1584.052329	18.274663	-0.052354	2.263028
277.536026	1576.113734	18.279667	-0.052341	2.258077
277.668721	1568.149312	18.284672	-0.052361	2.253115
277.545881	1560.206266	18.289677	-0.052333	2.248132
277.341262	1552.282357	18.294682	-0.052289	2.243143
277.378658	1544.359785	18.299687	-0.052291	2.238165
277.374590	1536.382898	18.304691	-0.052285	2.233138
277.222014	1528.440056	18.309696	-0.052251	2.228108
277.108602	1520.505566	18.314701	-0.052225	2.223075
277.244316	1512.532026	18.319706	-0.052245	2.218028
277.245540	1504.592237	18.324711	-0.052240	2.212980
277.033976	1496.661598	18.329715	-0.052195	2.207906
277.221268	1488.704832	18.334720	-0.052225	2.202840
277.106869	1480.775432	18.339725	-0.052199	2.197753
276.978633	1472.824626	18.344730	-0.052169	2.192638
277.010010	1464.855562	18.349735	-0.052170	2.187515
277.152076	1456.900810	18.354739	-0.052191	2.182399
277.111217	1448.971007	18.359744	-0.052178	2.177270
276.980763	1441.047842	18.364749	-0.052149	2.172125
276.788926	1433.102317	18.369754	-0.052108	2.166947
276.912940	1425.163005	18.374759	-0.052126	2.161791
276.763987	1417.248013	18.379763	-0.052093	2.156613
276.897474	1409.251947	18.384768	-0.052113	2.151395
276.882503	1401.321127	18.389773	-0.052105	2.146194
276.784047	1393.395152	18.394778	-0.052081	2.140975
276.635486	1385.487931	18.399783	-0.052048	2.135752
276.405643	1377.555167	18.404787	-0.052000	2.130490
276.441051	1369.601886	18.409792	-0.052001	2.125228
276.364177	1361.684897	18.414797	-0.051982	2.119966
276.234469	1353.757967	18.419802	-0.051953	2.114678
276.458210	1345.724188	18.424807	-0.051989	2.109341
276.351844	1337.790215	18.429811	-0.051964	2.104024
276.082817	1329.907342	18.434816	-0.051909	2.098713
276.257287	1321.953647	18.439821	-0.051936	2.093384
276.030796	1314.021109	18.444826	-0.051889	2.088016
276.028983	1306.103232	18.449831	-0.051883	2.082666
275.928306	1298.183013	18.454835	-0.051859	2.077292
276.121604	1290.201945	18.459840	-0.051890	2.071890
276.063592	1282.270173	18.464845	-0.051874	2.066484
275.941188	1274.359911	18.469850	-0.051846	2.061071
276.066175	1266.434536	18.474855	-0.051864	2.055659
275.824363	1258.508229	18.479859	-0.051814	2.050195
275.736610	1250.600557	18.484864	-0.051792	2.044745
275.951973	1242.655262	18.489869	-0.051827	2.039284
275.834134	1234.735665	18.494874	-0.051800	2.033793
275.795615	1226.788316	18.499879	-0.051787	2.028276
275.642987	1218.860596	18.504883	-0.051754	2.022746
275.627236	1210.950534	18.509888	-0.051746	2.017227
275.571503	1203.026339	18.514893	-0.051730	2.011679
275.451775	1195.085043	18.519898	-0.051702	2.006097
275.626376	1187.161085	18.524903	-0.051730	2.000542
275.326477	1179.288717	18.529907	-0.051669	1.994959
275.246431	1171.334743	18.534912	-0.051649	1.989325
275.187326	1163.423521	18.539917	-0.051632	1.983707
275.138329	1155.498376	18.544922	-0.051618	1.978065
275.204045	1147.568474	18.549927	-0.051625	1.972415
275.149335	1139.628862	18.554931	-0.051610	1.966730
274.860784	1131.755235	18.559936	-0.051551	1.961050
274.866687	1123.855985	18.564941	-0.051547	1.955367
274.719619	1115.881642	18.569946	-0.051514	1.949596
274.834956	1107.936401	18.574951	-0.051530	1.943858
274.897799	1100.011434	18.579955	-0.051537	1.938112
274.842548	1092.099402	18.584960	-0.051521	1.932346
274.834594	1084.177196	18.589965	-0.051515	1.926559
274.564324	1076.297491	18.594970	-0.051459	1.920758
274.433496	1068.413719	18.599975	-0.051430	1.914951
274.455761	1060.465423	18.604979	-0.051428	1.909096
274.571041	1052.536648	18.609984	-0.051445	1.903248
274.668264	1044.624338	18.614989	-0.051458	1.897393
274.428539	1036.738047	18.619994	-0.051408	1.891500
274.477154	1028.821175	18.624999	-0.051412	1.885599
274.393611	1020.931010	18.630003	-0.051391	1.879684
274.287768	1013.034449	18.635008	-0.051366	1.873743
274.306071	1005.095623	18.640013	-0.051364	1.867766
274.226698	997.188831	18.645018	-0.051344	1.861782
274.295201	989.293707	18.650023	-0.051352	1.855805
273.902730	981.417276	18.655027	-0.051273	1.849769
274.189674	973.477362	18.660032	-0.051322	1.843745
274.187930	965.592171	18.665037	-0.051316	1.837709
273.781638	957.720378	18.670042	-0.051235	1.831615
273.915800	949.785836	18.675047	-0.051255	1.825517
273.901882	941.898456	18.680051	-0.051247	1.819417
273.753903	934.019618	18.685056	-0.051215	1.813287
273.823373	926.102484	18.690061	-0.051222	1.807132
273.785419	918.211076	18.695066	-0.051210	1.800964
273.770857	910.335318	18.700071	-0.051202	1.794790
273.456253	902.412696	18.705075	-0.051138	1.788520
273.604886	894.490591	18.710080	-0.051161	1.782286
273.737733	886.602410	18.715085	-0.051180	1.776055
273.339842	878.747896	18.720090	-0.051101	1.769763
273.318591	870.859618	18.725095	-0.051092	1.763469
273.443499	862.964601	18.730099	-0.051110	1.757164
273.314034	855.080470	18.735104	-0.051081	1.750814
273.266867	847.201515	18.740109	-0.051067	1.744456
273.056188	839.339729	18.745114	-0.051022	1.738067
273.223876	831.430023	18.750119	-0.051048	1.731663
272.941610	823.572030	18.755123	-0.050991	1.725221
272.976748	815.703429	18.760128	-0.050992	1.718787
273.129516	807.804911	18.765133	-0.051015	1.712319
272.965399	799.918693	18.770138	-0.050980	1.705795
272.931944	792.066607	18.775143	-0.050968	1.699292
272.837845	784.198068	18.780147	-0.050945	1.692742
272.714808	776.319020	18.785152	-0.050917	1.686154
272.755534	768.455694	18.790157	-0.050920	1.679575
272.734082	760.579931	18.795162	-0.050911	1.672951
272.645675	752.702016	18.800167	-0.050889	1.666290
272.492452	744.861885	18.805171	-0.050855	1.659626
272.451949	737.002446	18.810176	-0.050843	1.652934
272.575024	729.106820	18.815181	-0.050860	1.646206
272.400166	721.280441	18.820186	-0.050823	1.639468
272.466787	713.391546	18.825191	-0.050830	1.632683
272.308575	705.509475	18.830195	-0.050795	1.625844
272.288196	697.656723	18.835200	-0.050786	1.619020
271.982031	689.852997	18.840205	-0.050724	1.612171
272.122784	681.951425	18.845210	-0.050745	1.605269
272.026130	674.139272	18.850215	-0.050722	1.598382
271.786319	666.307503	18.855219	-0.050672	1.591428
271.793509	658.444587	18.860224	-0.050668	1.584452
271.974334	650.584041	18.865229	-0.050697	1.577471
271.846842	642.727745	18.870234	-0.050668	1.570418
271.800292	634.911910	18.875239	-0.050654	1.563382
271.831353	627.070409	18.880243	-0.050655	1.556303
271.804844	619.209789	18.885248	-0.050645	1.549165
271.791359	611.378280	18.890253	-0.050637	1.542022
271.715507	603.558427	18.895258	-0.050618	1.534848
271.663159	595.730198	18.900263	-0.050603	1.527635
271.564813	587.914901	18.905267	-0.050579	1.520394
271.393718	580.121056	18.910272	-0.050542	1.513127
271.334919	572.286737	18.915277	-0.050526	1.505804
271.216074	564.482381	18.920282	-0.050499	1.498464
271.092653	556.675602	18.925287	-0.050471	1.491084
271.428807	548.792873	18.930291	-0.050528	1.483668
271.262296	541.021598	18.935296	-0.050492	1.476242
271.154024	533.182847	18.940301	-0.050467	1.468723
271.165273	525.358005	18.945306	-0.050464	1.461197
271.052025	517.586416	18.950311	-0.050438	1.453664
270.749565	509.816767	18.955315	-0.050376	1.446064
270.755828	502.016811	18.960320	-0.050372	1.438443
271.020569	494.170426	18.965325	-0.050416	1.430778
270.783558	486.406572	18.970330	-0.050367	1.423072
270.750136	478.635152	18.975335	-0.050356	1.415349
270.412042	470.881666	18.980339	-0.050288	1.407552
270.455483	463.088545	18.985344	-0.050291	1.399734
270.345543	455.322292	18.990349	-0.050265	1.391874
270.242253	447.527232	18.995354	-0.050241	1.383942
270.460237	439.723759	19.000359	-0.050276	1.376009
270.227936	431.976628	19.005363	-0.050228	1.368012
270.124588	424.228182	19.010368	-0.050203	1.359988
270.209767	416.456278	19.015373	-0.050214	1.351925
270.078672	408.693670	19.020378	-0.050185	1.343786
270.010122	400.965751	19.025383	-0.050167	1.335644
269.871603	393.220965	19.030387	-0.050136	1.327422
269.798070	385.494759	19.035392	-0.050117	1.319180
269.829596	377.662535	19.040397	-0.050118	1.310792
269.526865	369.910488	19.045402	-0.050056	1.302375
269.651270	362.174056	19.050407	-0.050074	1.293999
269.715848	354.426957	19.055411	-0.050081	1.285545
269.542288	346.753565	19.060416	-0.050044	1.277073
269.471878	339.040646	19.065421	-0.050026	1.268519
269.576424	331.304145	19.070426	-0.050040	1.259914
269.511124	323.620947	19.075431	-0.050023	1.251278
269.351593	315.943762	19.080435	-0.049988	1.242570
269.334395	308.259909	19.085440	-0.049980	1.233820
269.269331	300.561511	19.090445	-0.049963	1.224982
269.210726	292.881510	19.095450	-0.049947	1.216102
269.178720	285.206769	19.100455	-0.049936	1.207169
269.022509	277.569273	19.105459	-0.049902	1.198187
269.035479	269.888803	19.110464	-0.049899	1.189121
269.008162	262.236803	19.115469	-0.049889	1.180011
268.987313	254.577891	19.120474	-0.049880	1.170824
268.765262	246.978933	19.125479	-0.049834	1.161594
268.761343	239.325902	19.130483	-0.049828	1.152270
268.686610	231.672899	19.135488	-0.049809	1.142855
268.568878	224.074634	19.140493	-0.049782	1.133421
268.330086	216.482805	19.145498	-0.049733	1.123889
268.208028	208.900484	19.150503	-0.049705	1.114313
268.226922	201.278952	19.155507	-0.049703	1.104635
268.081597	193.712384	19.160512	-0.049671	1.094906
268.300975	186.086767	19.165517	-0.049707	1.085094
268.185547	178.541435	19.170522	-0.049681	1.075223
268.061161	170.987732	19.175527	-0.049653	1.065247
267.918849	163.458244	19.180531	-0.049621	1.055204
267.996789	155.890820	19.185536	-0.049631	1.045065
267.878519	148.393752	19.190541	-0.049604	1.034877
267.731809	140.878352	19.195546	-0.049571	1.024555
267.644330	133.394059	19.200551	-0.049550	1.014186
267.634475	125.895117	19.205555	-0.049543	1.003707
267.424081	118.438700	19.210560	-0.049499	0.993129
267.386116	110.946843	19.215565	-0.049487	0.982429
267.224373	103.504983	19.220570	-0.049452	0.971653
267.232844	96.062235	19.225575	-0.049449	0.960798
266.971054	88.671636	19.230579	-0.049395	0.949826
266.986287	81.250349	19.235584	-0.049393	0.938752
266.864364	73.868889	19.240589	-0.049366	0.927571
266.546938	66.542972	19.245594	-0.049302	0.916285
266.602627	59.381947	19.250599	-0.049308	0.905217