Fri Mar 12 11:46:31 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.594383	-0.020308	0.000000	0.000003	0.720878
0.668644	-0.033548	0.005005	-0.000011	0.720878
0.839592	-0.064759	0.010010	-0.000042	0.720876
0.892446	-0.070458	0.015014	-0.000052	0.720884
0.850773	-0.067653	0.020019	-0.000044	0.720875
0.828357	-0.060663	0.025024	-0.000040	0.720880
0.571736	-0.015535	0.030029	0.000008	0.720879
0.710045	-0.042599	0.035034	-0.000018	0.720874
0.876498	-0.070551	0.040038	-0.000049	0.720878
0.730154	-0.047639	0.045043	-0.000022	0.720871
0.734129	-0.042175	0.050048	-0.000023	0.720884
0.780190	-0.053883	0.055053	-0.000031	0.720877
0.829306	-0.063795	0.060058	-0.000040	0.720874
0.852633	-0.154184	0.065062	-0.000045	0.720704
0.714889	-0.214759	0.070067	-0.000019	0.720537
0.865127	-0.239586	0.075072	-0.000047	0.720541
1.042694	-0.272016	0.080077	-0.000080	0.720539
0.862752	-0.241731	0.085082	-0.000046	0.720535
0.854916	-0.235832	0.090086	-0.000045	0.720544
0.812849	-0.234501	0.095091	-0.000037	0.720532
0.841604	-0.389940	0.100096	-0.000042	0.720236
0.796030	-0.388973	0.105101	-0.000034	0.720222
0.908329	-0.409027	0.110106	-0.000054	0.720222
0.822990	-0.391110	0.115110	-0.000039	0.720227
0.822916	-0.395551	0.120115	-0.000039	0.720218
1.019260	-0.576691	0.125120	-0.000075	0.719930
0.889064	-0.568770	0.130125	-0.000051	0.719900
0.751827	-0.545652	0.135130	-0.000025	0.719898
0.773598	-0.546851	0.140134	-0.000029	0.719903
0.698374	-0.641155	0.145139	-0.000015	0.719690
0.627690	-0.673048	0.150144	-0.000002	0.719603
0.523411	-0.655918	0.155149	0.000018	0.719600
0.683285	-0.684802	0.160154	-0.000012	0.719599
0.700990	-0.812867	0.165158	-0.000015	0.719353
0.482611	-0.818950	0.170163	0.000025	0.719264
0.658502	-0.846214	0.175168	-0.000007	0.719272
0.562734	-0.869974	0.180173	0.000011	0.719191
0.611107	-0.996745	0.185178	0.000002	0.718958
0.636749	-0.998162	0.190182	-0.000003	0.718964
0.616112	-1.006369	0.195187	0.000001	0.718941
0.632763	-1.158016	0.200192	-0.000002	0.718647
0.772594	-1.182897	0.205197	-0.000028	0.718647
0.523805	-1.157146	0.210202	0.000018	0.718611
0.509080	-1.282346	0.215206	0.000021	0.718358
0.468941	-1.280904	0.220211	0.000028	0.718347
0.677331	-1.366134	0.225216	-0.000010	0.718252
0.710148	-1.488953	0.230221	-0.000016	0.718021
0.537921	-1.460584	0.235226	0.000016	0.718016
0.461706	-1.552412	0.240230	0.000030	0.717808
0.232784	-1.565836	0.245235	0.000073	0.717701
0.218772	-1.574609	0.250240	0.000075	0.717678
-0.040711	-1.678427	0.255245	0.000124	0.717382
0.088915	-1.703189	0.260250	0.000100	0.717378
0.332249	-1.820666	0.265254	0.000054	0.717232
0.264876	-1.886257	0.270259	0.000067	0.717078
0.161716	-1.887466	0.275264	0.000086	0.717039
0.153226	-2.029507	0.280269	0.000088	0.716755
0.092051	-2.020085	0.285274	0.000099	0.716752
0.119980	-2.152787	0.290278	0.000094	0.716499
0.208891	-2.196274	0.295283	0.000078	0.716445
0.070968	-2.272030	0.300288	0.000104	0.716246
-0.398419	-2.245805	0.305293	0.000191	0.716132
-0.584119	-2.262186	0.310298	0.000226	0.716034
-0.505662	-2.350156	0.315302	0.000211	0.715888
-0.760516	-2.326395	0.320307	0.000259	0.715845
-0.329352	-2.550925	0.325312	0.000178	0.715552
-0.422932	-2.538167	0.330317	0.000196	0.715544
-1.068949	-2.579989	0.335322	0.000316	0.715233
-1.488684	-2.502318	0.340326	0.000394	0.715238
-3.837759	-2.186895	0.345331	0.000832	0.715034
-3.883555	-2.240311	0.350336	0.000840	0.714912
-3.900457	-2.238416	0.355341	0.000843	0.714909
-4.549395	-2.126008	0.360346	0.000964	0.714903
-4.622820	-2.248842	0.365350	0.000978	0.714633
-4.890843	-2.216951	0.370355	0.001028	0.714602
-4.772677	-2.234637	0.375360	0.001006	0.714608
-4.927550	-2.219798	0.380365	0.001035	0.714583
-5.944806	-2.195363	0.385370	0.001224	0.714272
-5.653513	-2.243620	0.390374	0.001170	0.714279
-6.179292	-2.154797	0.395379	0.001268	0.714269
-5.844270	-2.209783	0.400384	0.001205	0.714278
-5.740883	-2.316188	0.405389	0.001186	0.714104
-7.136357	-2.136835	0.410394	0.001446	0.713966
-6.526026	-2.240679	0.415398	0.001333	0.713976
-6.641153	-2.224621	0.420403	0.001354	0.713967
-6.756957	-2.202315	0.425408	0.001376	0.713970
-7.223860	-2.257921	0.430413	0.001463	0.713694
-7.660978	-2.204516	0.435418	0.001544	0.713645
-7.310772	-2.262803	0.440422	0.001479	0.713653
-7.495270	-2.234265	0.445427	0.001513	0.713645
-7.662000	-2.201787	0.450432	0.001544	0.713650
-7.558851	-2.332952	0.455437	0.001525	0.713426
-8.623568	-2.178939	0.460442	0.001723	0.713355
-8.682982	-2.162639	0.465446	0.001734	0.713366
-8.555420	-2.191661	0.470451	0.001711	0.713354
-8.743218	-2.154134	0.475456	0.001746	0.713362
-8.953238	-2.117750	0.480461	0.001785	0.713360
-9.407484	-2.198743	0.485466	0.001869	0.713037
-9.438964	-2.199189	0.490470	0.001875	0.713025
-9.820329	-2.135373	0.495475	0.001946	0.713017
-9.564058	-2.177479	0.500480	0.001899	0.713024
-9.649343	-2.164770	0.505485	0.001915	0.713019
-9.805358	-2.139732	0.510490	0.001944	0.713013
-9.627355	-2.220251	0.515494	0.001910	0.712916
-10.772704	-2.123900	0.520499	0.002124	0.712702
-10.130849	-2.235575	0.525504	0.002004	0.712707
-10.644677	-2.146076	0.530509	0.002100	0.712703
-10.851939	-2.109670	0.535514	0.002139	0.712702
-10.080264	-2.241144	0.540518	0.001995	0.712714
-10.747143	-2.128138	0.545523	0.002119	0.712702
-11.086969	-2.176727	0.550528	0.002182	0.712485
-11.257922	-2.196090	0.555533	0.002214	0.712386
-11.220172	-2.206280	0.560538	0.002207	0.712379
-11.451268	-2.161787	0.565542	0.002250	0.712385
-11.569356	-2.144601	0.570547	0.002272	0.712377
-11.208167	-2.203644	0.575552	0.002205	0.712388
-11.472190	-2.156458	0.580557	0.002254	0.712388
-12.467151	-2.121047	0.585562	0.002440	0.712106
-12.140368	-2.186301	0.590566	0.002379	0.712091
-12.315757	-2.157493	0.595571	0.002411	0.712087
-12.499499	-2.123083	0.600576	0.002446	0.712090
-12.202650	-2.176658	0.605581	0.002390	0.712088
-12.317253	-2.157702	0.610586	0.002412	0.712085
-12.263626	-2.162533	0.615590	0.002402	0.712095
-12.943629	-2.185685	0.620595	0.002528	0.711807
-13.119168	-2.178420	0.625600	0.002561	0.711759
-13.257110	-2.152172	0.630605	0.002587	0.711763
-13.418476	-2.126212	0.635610	0.002617	0.711757
-13.213509	-2.158835	0.640614	0.002579	0.711765
-13.279673	-2.151641	0.645619	0.002591	0.711755
-13.330807	-2.139373	0.650624	0.002601	0.711762
-13.245971	-2.256396	0.655629	0.002585	0.711558
-14.214159	-2.139301	0.660634	0.002765	0.711448
-14.289711	-2.120257	0.665638	0.002779	0.711459
-14.670755	-2.057303	0.670643	0.002850	0.711449
-14.161738	-2.145400	0.675648	0.002756	0.711454
-13.911266	-2.189538	0.680653	0.002709	0.711455
-14.499896	-2.086306	0.685658	0.002819	0.711452
-14.067821	-2.231397	0.690662	0.002738	0.711316
-15.068192	-2.143786	0.695667	0.002924	0.711135
-14.948064	-2.164191	0.700672	0.002902	0.711137
-14.888883	-2.172913	0.705677	0.002891	0.711140
-15.097522	-2.138839	0.710682	0.002930	0.711134
-15.073129	-2.138194	0.715686	0.002925	0.711144
-15.464777	-2.074207	0.720691	0.002998	0.711132
-15.030957	-2.198616	0.725696	0.002918	0.711038
-15.594308	-2.181453	0.730701	0.003023	0.710872
-15.975361	-2.115988	0.735706	0.003094	0.710867
-15.841406	-2.136863	0.740710	0.003069	0.710873
-15.701872	-2.163972	0.745715	0.003043	0.710869
-15.880872	-2.129586	0.750720	0.003076	0.710874
-16.096440	-2.091343	0.755725	0.003116	0.710873
-15.979565	-2.214411	0.760730	0.003095	0.710669
-16.726953	-2.146897	0.765734	0.003234	0.710538
-17.135275	-2.077781	0.770739	0.003310	0.710531
-16.769408	-2.141745	0.775744	0.003242	0.710533
-16.619771	-2.167136	0.780749	0.003214	0.710535
-17.068888	-2.089109	0.785754	0.003297	0.710531
-16.918810	-2.112273	0.790758	0.003269	0.710539
-16.533662	-2.247429	0.795763	0.003198	0.710406
-17.795474	-2.116923	0.800768	0.003433	0.710217
-17.674198	-2.136285	0.805773	0.003410	0.710221
-17.778793	-2.121253	0.810778	0.003430	0.710214
-17.438595	-2.174981	0.815782	0.003366	0.710228
-17.737635	-2.128617	0.820787	0.003422	0.710214
-17.762520	-2.122479	0.825792	0.003427	0.710217
-17.592240	-2.226929	0.830797	0.003395	0.710069
-19.098797	-2.048849	0.835802	0.003676	0.709889
-18.369780	-2.173709	0.840806	0.003540	0.709899
-18.610497	-2.133558	0.845811	0.003585	0.709893
-18.815541	-2.094923	0.850816	0.003623	0.709897
-18.438221	-2.163079	0.855821	0.003553	0.709895
-18.558999	-2.144536	0.860826	0.003575	0.709889
-18.325062	-2.239178	0.865830	0.003532	0.709783
-19.620560	-2.104835	0.870835	0.003773	0.709590
-19.486631	-2.125596	0.875840	0.003748	0.709596
-19.041077	-2.203417	0.880845	0.003665	0.709600
-19.526111	-2.119253	0.885850	0.003755	0.709595
-19.433577	-2.132325	0.890854	0.003738	0.709602
-19.442851	-2.134433	0.895859	0.003740	0.709594
-19.238164	-2.247914	0.900864	0.003702	0.709440
-20.763803	-2.063373	0.905869	0.003986	0.709265
-20.357844	-2.138352	0.910874	0.003910	0.709260
-20.236297	-2.153671	0.915878	0.003888	0.709273
-20.515537	-2.109653	0.920883	0.003940	0.709261
-20.228284	-2.159224	0.925888	0.003886	0.709264
-20.028521	-2.194295	0.930893	0.003849	0.709265
-20.617502	-2.136572	0.935898	0.003959	0.709171
-21.209593	-2.134669	0.940902	0.004069	0.708963
-20.907424	-2.194035	0.945907	0.004013	0.708952
-21.155598	-2.145608	0.950912	0.004059	0.708961
-20.987310	-2.175850	0.955917	0.004028	0.708960
-21.013536	-2.174115	0.960922	0.004033	0.708954
-20.908570	-2.189133	0.965926	0.004013	0.708961
-21.481713	-2.177712	0.970931	0.004120	0.708780
-22.569432	-2.053393	0.975936	0.004323	0.708640
-21.920102	-2.168435	0.980941	0.004202	0.708642
-22.141048	-2.131604	0.985946	0.004243	0.708637
-22.255964	-2.107474	0.990950	0.004264	0.708644
-22.032468	-2.152233	0.995955	0.004223	0.708634
-22.101186	-2.137584	1.000960	0.004236	0.708639
-22.343815	-2.112904	1.005965	0.004281	0.708601
-23.067058	-2.109970	1.010970	0.004415	0.708349
-22.598624	-2.190008	1.015974	0.004328	0.708356
-22.971186	-2.126191	1.020979	0.004398	0.708351
-22.963415	-2.125604	1.025984	0.004396	0.708355
-22.752728	-2.162625	1.030989	0.004357	0.708356
-23.104288	-2.104499	1.035994	0.004422	0.708346
-22.964081	-2.163779	1.040998	0.004396	0.708278
-23.958657	-2.120520	1.046003	0.004582	0.708009
-23.655774	-2.172768	1.051008	0.004525	0.708012
-24.112224	-2.088039	1.056013	0.004610	0.708019
-24.204860	-2.074657	1.061018	0.004627	0.708013
-23.749095	-2.151429	1.066022	0.004543	0.708022
-24.184658	-2.078248	1.071027	0.004624	0.708013
-24.111461	-2.091232	1.076032	0.004610	0.708013
-23.947718	-2.226352	1.081037	0.004580	0.707800
-25.027927	-2.084735	1.086042	0.004781	0.707698
-24.847424	-2.113265	1.091046	0.004747	0.707705
-24.793322	-2.126503	1.096051	0.004737	0.707698
-24.807497	-2.122512	1.101056	0.004740	0.707701
-24.935919	-2.096329	1.106061	0.004764	0.707708
-25.044392	-2.082224	1.111066	0.004784	0.707697
-24.898295	-2.178669	1.116070	0.004757	0.707556
-25.857107	-2.097916	1.121075	0.004935	0.707375
-25.550780	-2.150626	1.126080	0.004878	0.707379
-25.606139	-2.139062	1.131085	0.004889	0.707382
-26.036032	-2.066301	1.136090	0.004969	0.707374
-25.831665	-2.098581	1.141094	0.004931	0.707382
-25.789935	-2.108018	1.146099	0.004923	0.707378
-25.908386	-2.128497	1.151104	0.004945	0.707295
-26.343126	-2.154612	1.156109	0.005026	0.707087
-26.653502	-2.105912	1.161114	0.005084	0.707074
-26.386603	-2.147552	1.166118	0.005034	0.707085
-26.574979	-2.116205	1.171123	0.005069	0.707081
-26.756985	-2.083817	1.176128	0.005103	0.707081
-26.667854	-2.097580	1.181133	0.005087	0.707085
-26.495828	-2.176893	1.186138	0.005055	0.706987
-27.485236	-2.115049	1.191142	0.005239	0.706757
-27.493569	-2.117697	1.196147	0.005241	0.706749
-27.725556	-2.075543	1.201152	0.005284	0.706750
-27.362599	-2.136447	1.206157	0.005216	0.706758
-27.784753	-2.064748	1.211162	0.005295	0.706751
-27.351346	-2.137472	1.216166	0.005214	0.706760
-27.498561	-2.125740	1.221171	0.005242	0.706731
-28.415612	-2.102344	1.226176	0.005412	0.706449
-28.351416	-2.113025	1.231181	0.005400	0.706451
-28.823035	-2.033865	1.236186	0.005488	0.706441
-28.291388	-2.125347	1.241190	0.005389	0.706447
-28.454823	-2.099413	1.246195	0.005420	0.706441
-28.323444	-2.120789	1.251200	0.005395	0.706445
-28.353997	-2.110929	1.256205	0.005401	0.706454
-29.287392	-2.073803	1.261210	0.005575	0.706194
-29.439030	-2.076450	1.266214	0.005603	0.706134
-29.366389	-2.092364	1.271219	0.005590	0.706128
-29.433786	-2.080132	1.276224	0.005602	0.706129
-29.354152	-2.092051	1.281229	0.005587	0.706133
-29.388940	-2.087883	1.286234	0.005594	0.706129
-29.442167	-2.076468	1.291238	0.005604	0.706133
-29.695743	-2.056399	1.296243	0.005651	0.706082
-30.029555	-2.105551	1.301248	0.005713	0.705864
-29.758070	-2.150314	1.306253	0.005663	0.705871
-30.595438	-2.006489	1.311258	0.005819	0.705860
-30.051285	-2.099626	1.316262	0.005717	0.705868
-29.945889	-2.121572	1.321267	0.005698	0.705861
-30.309232	-2.055147	1.326272	0.005765	0.705865
-30.078550	-2.161865	1.331277	0.005723	0.705733
-31.236656	-2.061534	1.336282	0.005938	0.705519
-30.768036	-2.140783	1.341286	0.005851	0.705528
-31.010844	-2.098560	1.346291	0.005896	0.705525
-31.079386	-2.086471	1.351296	0.005909	0.705525
-30.718601	-2.148048	1.356301	0.005842	0.705531
-31.286305	-2.050350	1.361306	0.005948	0.705523
-31.003461	-2.196856	1.366310	0.005895	0.705330
-31.866210	-2.102199	1.371315	0.006056	0.705211
-32.139716	-2.053300	1.376320	0.006107	0.705211
-31.909103	-2.091713	1.381325	0.006064	0.705217
-32.020584	-2.076118	1.386330	0.006084	0.705208
-31.766241	-2.119459	1.391334	0.006037	0.705212
-32.125944	-2.055116	1.396339	0.006104	0.705212
-32.246539	-2.136670	1.401344	0.006127	0.705005
-32.676417	-2.117641	1.406349	0.006207	0.704889
-32.913741	-2.077749	1.411354	0.006251	0.704884
-32.789897	-2.096431	1.416358	0.006228	0.704891
-32.842250	-2.090329	1.421363	0.006238	0.704884
-32.983004	-2.065366	1.426368	0.006264	0.704884
-32.740774	-2.106201	1.431373	0.006219	0.704888
-33.034502	-2.134060	1.436378	0.006274	0.704727
-33.800530	-2.064489	1.441382	0.006416	0.704592
-33.690706	-2.086794	1.446387	0.006396	0.704586
-33.884301	-2.051830	1.451392	0.006432	0.704587
-33.465291	-2.123369	1.456397	0.006354	0.704593
-33.881451	-2.053723	1.461402	0.006431	0.704584
-33.638684	-2.092524	1.466406	0.006386	0.704593
-33.301747	-2.239676	1.471411	0.006324	0.704418
-34.545644	-2.096956	1.476416	0.006555	0.704258
-34.139054	-2.167136	1.481421	0.006479	0.704263
-34.673769	-2.075730	1.486426	0.006579	0.704255
-34.482784	-2.105729	1.491430	0.006543	0.704263
-34.575322	-2.090561	1.496435	0.006561	0.704260
-34.744383	-2.061829	1.501440	0.006592	0.704257
-34.694936	-2.192440	1.506445	0.006583	0.704012
-35.833379	-2.020445	1.511450	0.006795	0.703949
-35.504290	-2.075649	1.516454	0.006734	0.703956
-35.209192	-2.129282	1.521459	0.006679	0.703954
-35.327306	-2.107658	1.526464	0.006701	0.703955
-35.218878	-2.125726	1.531469	0.006681	0.703958
-35.312187	-2.113788	1.536474	0.006698	0.703948
-35.775930	-2.174084	1.541478	0.006785	0.703660
-36.200232	-2.110828	1.546483	0.006864	0.703635
-36.381836	-2.079082	1.551488	0.006897	0.703633
-35.768190	-2.186029	1.556493	0.006783	0.703638
-36.323579	-2.091703	1.561498	0.006887	0.703629
-36.425329	-2.068122	1.566502	0.006906	0.703640
-35.786838	-2.216708	1.571507	0.006787	0.703569
-36.992408	-2.113691	1.576512	0.007011	0.703343
-36.864614	-2.132315	1.581517	0.006987	0.703352
-37.317956	-2.057029	1.586522	0.007072	0.703341
-36.834040	-2.138916	1.591526	0.006982	0.703349
-37.052030	-2.102615	1.596531	0.007022	0.703344
-37.432522	-2.037342	1.601536	0.007093	0.703339
-36.799854	-2.218625	1.606541	0.006976	0.703201
-38.121274	-2.080819	1.611546	0.007222	0.703003
-38.084838	-2.082306	1.616550	0.007215	0.703013
-38.043995	-2.093081	1.621555	0.007207	0.703006
-38.228082	-2.061316	1.626560	0.007241	0.703004
-37.819128	-2.129377	1.631565	0.007165	0.703014
-38.111788	-2.082427	1.636570	0.007220	0.703003
-37.951866	-2.154235	1.641574	0.007190	0.702916
-39.019687	-2.073226	1.646579	0.007389	0.702694
-38.843223	-2.106790	1.651584	0.007356	0.702690
-38.895293	-2.093967	1.656589	0.007366	0.702697
-38.905264	-2.096413	1.661594	0.007368	0.702689
-38.950977	-2.083526	1.666598	0.007376	0.702698
-38.788099	-2.115672	1.671603	0.007346	0.702692
-38.933472	-2.117499	1.676608	0.007373	0.702636
-39.768704	-2.096483	1.681613	0.007529	0.702377
-39.765688	-2.102363	1.686618	0.007528	0.702366
-39.537085	-2.138081	1.691622	0.007486	0.702377
-39.816499	-2.090243	1.696627	0.007538	0.702372
-40.274763	-2.010128	1.701632	0.007623	0.702369
-39.761948	-2.097218	1.706637	0.007528	0.702378
-39.858538	-2.085415	1.711642	0.007546	0.702367
-40.384181	-2.118660	1.716646	0.007643	0.702110
-40.800977	-2.062957	1.721651	0.007721	0.702072
-40.556395	-2.107470	1.726656	0.007676	0.702071
-40.421107	-2.128327	1.731661	0.007650	0.702077
-40.775333	-2.069309	1.736666	0.007716	0.702069
-40.600897	-2.096220	1.741670	0.007684	0.702077
-40.632592	-2.093439	1.746675	0.007690	0.702071
-41.446404	-2.101125	1.751680	0.007841	0.701762
-41.232557	-2.147256	1.756685	0.007802	0.701746
-41.608436	-2.084527	1.761690	0.007872	0.701737
-41.601578	-2.082408	1.766694	0.007870	0.701744
-41.552716	-2.091598	1.771699	0.007861	0.701743
-41.452490	-2.111143	1.776704	0.007843	0.701739
-41.607214	-2.078669	1.781709	0.007871	0.701749
-42.129014	-2.124624	1.786714	0.007969	0.701468
-42.110090	-2.142509	1.791718	0.007965	0.701438
-42.033334	-2.156403	1.796723	0.007951	0.701438
-42.390107	-2.094803	1.801728	0.008017	0.701434
-42.278228	-2.111529	1.806733	0.007997	0.701440
-42.401967	-2.092987	1.811738	0.008020	0.701433
-42.610870	-2.086514	1.816742	0.008059	0.701371
-43.186427	-2.105846	1.821747	0.008166	0.701124
-42.997027	-2.141677	1.826752	0.008131	0.701120
-43.232809	-2.096140	1.831757	0.008174	0.701127
-43.584332	-2.038171	1.836762	0.008240	0.701117
-43.209674	-2.103030	1.841766	0.008170	0.701121
-43.162123	-2.111061	1.846771	0.008161	0.701122
-43.670601	-2.024988	1.851776	0.008256	0.701112
-43.487866	-2.171904	1.856781	0.008222	0.700881
-43.827154	-2.116075	1.861786	0.008285	0.700871
-44.059531	-2.072109	1.866790	0.008329	0.700876
-43.834223	-2.112532	1.871795	0.008287	0.700876
-43.724905	-2.134968	1.876800	0.008266	0.700870
-43.712613	-2.133014	1.881805	0.008264	0.700878
-44.629013	-2.108530	1.886810	0.008435	0.700596
-44.878328	-2.092462	1.891814	0.008481	0.700539
-44.837512	-2.101834	1.896819	0.008474	0.700535
-45.062223	-2.062661	1.901824	0.008515	0.700533
-45.007548	-2.068460	1.906829	0.008505	0.700541
-44.690139	-2.129467	1.911834	0.008446	0.700532
-44.733687	-2.118673	1.916838	0.008454	0.700538
-45.429006	-2.139006	1.921843	0.008584	0.700245
-45.757847	-2.094693	1.926848	0.008645	0.700216
-45.688965	-2.104336	1.931853	0.008632	0.700221
-45.908056	-2.070782	1.936858	0.008673	0.700210
-45.786581	-2.087957	1.941862	0.008650	0.700219
-45.550939	-2.129955	1.946867	0.008607	0.700219
-45.713530	-2.117868	1.951872	0.008637	0.700185
-46.308423	-2.151531	1.956877	0.008748	0.699901
-46.403696	-2.139863	1.961882	0.008766	0.699890
-46.712430	-2.082433	1.966886	0.008823	0.699895
-46.609686	-2.101694	1.971891	0.008804	0.699893
-46.509241	-2.120890	1.976896	0.008785	0.699890
-46.425672	-2.133231	1.981901	0.008770	0.699896
-46.832102	-2.114303	1.986906	0.008845	0.699787
-47.582720	-2.072819	1.991910	0.008985	0.699599
-47.012367	-2.174896	1.996915	0.008879	0.699599
-47.601027	-2.070008	2.001920	0.008989	0.699598
-47.130140	-2.154708	2.011917	0.008901	0.699597
-47.521537	-2.085281	2.021914	0.008974	0.699596
-47.887496	-2.137286	2.031910	0.009042	0.699358
-48.271491	-2.113932	2.041907	0.009114	0.699266
-48.244678	-2.119781	2.051904	0.009109	0.699264
-47.594368	-2.157013	2.061901	0.008988	0.699423
-47.904791	-2.082474	2.071898	0.009046	0.699462
-47.298289	-2.125150	2.081894	0.008933	0.699595
-47.306569	-2.122893	2.091891	0.008934	0.699597
-47.506846	-2.087512	2.101888	0.008972	0.699596
-47.330703	-2.119108	2.111885	0.008939	0.699595
-47.485548	-2.090521	2.121882	0.008968	0.699597
-47.266116	-2.129644	2.131878	0.008927	0.699597
-47.346553	-2.114673	2.141875	0.008942	0.699598
-47.508168	-2.046147	2.151872	0.008972	0.699679
-46.560520	-2.109472	2.161869	0.008796	0.699893
-46.583136	-2.105351	2.171866	0.008800	0.699893
-46.288096	-2.157958	2.181862	0.008745	0.699893
-46.551410	-2.110797	2.191859	0.008794	0.699894
-45.971205	-2.106437	2.201856	0.008686	0.700112
-45.696027	-2.101635	2.211853	0.008635	0.700221
-45.717626	-2.097735	2.221850	0.008639	0.700221
-45.347227	-2.163856	2.231846	0.008570	0.700221
-45.336046	-2.084177	2.241843	0.008568	0.700387
-44.779292	-2.107977	2.251840	0.008465	0.700540
-44.906599	-2.087462	2.261837	0.008488	0.700535
-44.838286	-2.099287	2.271834	0.008476	0.700536
-44.198650	-2.069590	2.281830	0.008357	0.700827
-44.093855	-2.062502	2.291827	0.008337	0.700879
-43.688801	-2.134994	2.301824	0.008262	0.700878
-44.100441	-2.035734	2.311821	0.008338	0.700931
-43.397000	-2.066837	2.321818	0.008207	0.701122
-43.110284	-2.117106	2.331814	0.008154	0.701123
-43.117031	-2.114426	2.341811	0.008155	0.701126
-42.456625	-2.102082	2.351808	0.008033	0.701390
-42.337401	-2.099321	2.361805	0.008010	0.701438
-42.293884	-2.107109	2.371802	0.008002	0.701438
-42.175701	-2.078757	2.381798	0.007980	0.701538
-41.528124	-2.090963	2.391795	0.007860	0.701747
-41.288893	-2.134113	2.401792	0.007815	0.701746
-41.805845	-2.041228	2.411789	0.007912	0.701747
-40.760091	-2.069420	2.421786	0.007717	0.702067
-40.573658	-2.099330	2.431782	0.007682	0.702074
-40.407922	-2.127443	2.441779	0.007652	0.702077
-40.298345	-2.075942	2.451776	0.007631	0.702220
-39.677970	-2.111872	2.461773	0.007516	0.702371
-39.800582	-2.089961	2.471770	0.007539	0.702371
-40.019289	-2.029421	2.481766	0.007579	0.702415
-38.800682	-2.105827	2.491763	0.007353	0.702699
-38.690015	-2.127676	2.501760	0.007332	0.702695
-38.990936	-2.073896	2.511757	0.007388	0.702695
-38.605420	-2.051955	2.521754	0.007316	0.702878
-38.064447	-2.083671	2.531750	0.007216	0.703009
-38.117725	-2.074240	2.541747	0.007226	0.703009
-37.875719	-2.073342	2.551744	0.007181	0.703097
-37.275508	-2.059971	2.561741	0.007069	0.703340
-36.916478	-2.123200	2.571738	0.007002	0.703342
-37.292360	-2.055011	2.581734	0.007072	0.703344
-36.583061	-2.073359	2.591731	0.006940	0.703562
-36.327315	-2.082388	2.601728	0.006893	0.703636
-36.596108	-2.035229	2.611725	0.006943	0.703634
-35.892397	-2.105877	2.621722	0.006812	0.703745
-35.527236	-2.068342	2.631718	0.006744	0.703952
-35.373504	-2.094655	2.641715	0.006715	0.703954
-35.449352	-2.080890	2.651712	0.006729	0.703954
-34.665242	-2.082043	2.661709	0.006583	0.704234
-34.362015	-2.124115	2.671706	0.006527	0.704258
-34.332202	-2.128839	2.681702	0.006521	0.704259
-34.431645	-2.076131	2.691699	0.006540	0.704329
-33.590182	-2.096543	2.701696	0.006383	0.704590
-33.575557	-2.099839	2.711693	0.006381	0.704589
-33.642103	-2.088818	2.721690	0.006393	0.704587
-33.246079	-2.051687	2.731686	0.006319	0.704804
-32.600129	-2.125668	2.741683	0.006199	0.704887
-32.691731	-2.109794	2.751680	0.006216	0.704886
-32.701901	-2.081080	2.761677	0.006218	0.704940
-32.066885	-2.060682	2.771674	0.006100	0.705209
-31.822917	-2.103505	2.781670	0.006055	0.705210
-32.003415	-2.071628	2.791667	0.006088	0.705209
-31.450055	-2.034831	2.801664	0.005985	0.705482
-31.101296	-2.075012	2.811661	0.005920	0.705526
-30.763848	-2.134187	2.821658	0.005858	0.705528
-31.056476	-2.023203	2.831654	0.005912	0.705646
-29.913882	-2.116654	2.841651	0.005700	0.705868
-30.059190	-2.092489	2.851648	0.005727	0.705864
-30.075804	-2.090645	2.861645	0.005730	0.705862
-29.570779	-2.072734	2.871642	0.005636	0.706079
-29.283683	-2.096342	2.881638	0.005582	0.706134
-29.061685	-2.136178	2.891635	0.005541	0.706134
-29.375513	-2.029491	2.901632	0.005600	0.706235
-28.555544	-2.071393	2.911629	0.005447	0.706445
-28.513742	-2.078524	2.921626	0.005439	0.706445
-28.688886	-2.032553	2.931622	0.005472	0.706475
-27.592863	-2.088684	2.941619	0.005268	0.706755
-27.702971	-2.068970	2.951616	0.005288	0.706755
-27.633332	-2.082969	2.961613	0.005276	0.706751
-27.095698	-2.064807	2.971610	0.005175	0.706980
-26.609827	-2.100760	2.981606	0.005085	0.707082
-26.620887	-2.098896	2.991603	0.005087	0.707081
-26.847523	-2.034469	3.001600	0.005129	0.707130
-25.792366	-2.098907	3.011597	0.004933	0.707378
-25.897211	-2.080248	3.021594	0.004953	0.707378
-25.869188	-2.085194	3.031590	0.004947	0.707378
-25.284219	-2.074541	3.041587	0.004839	0.707608
-25.064519	-2.066469	3.051584	0.004798	0.707703
-24.878233	-2.101339	3.061581	0.004763	0.707699
-24.810761	-2.092042	3.071578	0.004751	0.707742
-23.974497	-2.103582	3.081574	0.004595	0.708017
-23.851472	-2.124526	3.091571	0.004572	0.708019
-24.127001	-2.076966	3.101568	0.004623	0.708016
-23.616775	-2.082358	3.111565	0.004528	0.708188
-23.360142	-2.046896	3.121562	0.004481	0.708350
-23.258562	-2.063042	3.131558	0.004462	0.708354
-23.202103	-2.051175	3.141555	0.004451	0.708398
-22.447787	-2.062174	3.151552	0.004311	0.708645
-22.243321	-2.101065	3.161549	0.004273	0.708640
-22.491677	-2.057025	3.171546	0.004319	0.708639
-21.633526	-2.103463	3.181542	0.004159	0.708853
-21.511623	-2.071585	3.191539	0.004137	0.708960
-21.416601	-2.088706	3.201536	0.004119	0.708959
-21.439587	-2.066096	3.211533	0.004123	0.708996
-20.979343	-2.013361	3.221530	0.004038	0.709266
-20.401709	-2.117666	3.231526	0.003930	0.709263
-20.532325	-2.092191	3.241523	0.003955	0.709268
-20.095537	-2.050340	3.251520	0.003873	0.709507
-19.632966	-2.087446	3.261517	0.003787	0.709597
-19.740983	-2.068420	3.271514	0.003808	0.709597
-19.453965	-2.094202	3.281510	0.003754	0.709648
-19.020003	-2.045133	3.291507	0.003673	0.709900
-18.640212	-2.114097	3.301504	0.003603	0.709898
-18.812929	-2.085301	3.311501	0.003635	0.709893
-18.714381	-1.993773	3.321498	0.003617	0.710111
-17.827680	-2.097268	3.331494	0.003452	0.710220
-18.137503	-2.040676	3.341491	0.003509	0.710223
-17.816033	-2.048439	3.351488	0.003449	0.710322
-17.054012	-2.077150	3.361485	0.003308	0.710536
-16.995505	-2.088427	3.371482	0.003297	0.710534
-16.920910	-2.099951	3.381478	0.003283	0.710537
-16.387915	-2.080258	3.391475	0.003184	0.710766
-16.118280	-2.073926	3.401472	0.003134	0.710875
-16.212569	-2.056566	3.411469	0.003151	0.710876
-16.155893	-2.055225	3.421466	0.003141	0.710898
-15.388541	-2.069868	3.431462	0.002998	0.711142
-15.369551	-2.073635	3.441459	0.002994	0.711141
-15.031808	-2.134202	3.451456	0.002932	0.711140
-15.173145	-2.010262	3.461453	0.002958	0.711337
-14.490027	-2.071686	3.471450	0.002831	0.711457
-14.730465	-2.029107	3.481446	0.002876	0.711457
-14.351449	-2.043659	3.491443	0.002805	0.711562
-13.600753	-2.076142	3.501440	0.002665	0.711764
-13.913512	-2.022401	3.511437	0.002724	0.711760
-13.549658	-2.086482	3.521434	0.002656	0.711762
-12.699289	-2.074813	3.531430	0.002498	0.712087
-12.675539	-2.075388	3.541427	0.002493	0.712094
-12.566781	-2.095739	3.551424	0.002473	0.712092
-12.683453	-2.034151	3.561421	0.002495	0.712173
-11.725609	-2.097484	3.571418	0.002317	0.712387
-11.522385	-2.132783	3.581414	0.002279	0.712389
-11.622447	-2.114042	3.591411	0.002298	0.712390
-11.272900	-2.079194	3.601408	0.002232	0.712584
-10.906325	-2.080170	3.611405	0.002164	0.712712
-10.939301	-2.073931	3.621402	0.002170	0.712712
-10.949508	-2.052986	3.631398	0.002172	0.712750
-9.877659	-2.103900	3.641395	0.001973	0.713029
-9.453223	-2.179121	3.651392	0.001894	0.713030
-9.881848	-2.103017	3.661389	0.001974	0.713029
-9.709793	-2.108882	3.671386	0.001942	0.713078
-8.841628	-2.119071	3.681382	0.001780	0.713366
-8.670930	-2.149121	3.691379	0.001748	0.713366
-8.719453	-2.141842	3.701376	0.001758	0.713363
-8.778782	-2.090357	3.711373	0.001769	0.713445
-7.441761	-2.224410	3.721370	0.001520	0.713652
-7.685386	-2.178951	3.731366	0.001565	0.713656
-7.505820	-2.209047	3.741363	0.001532	0.713659
-7.616400	-2.179863	3.751360	0.001552	0.713678
-6.904333	-2.160336	3.761357	0.001420	0.713969
-6.781440	-2.180177	3.771354	0.001397	0.713973
-6.779861	-2.179662	3.781350	0.001397	0.713974
-6.563853	-2.194619	3.791347	0.001357	0.714021
-6.009296	-2.162888	3.801344	0.001253	0.714280
-5.988513	-2.167250	3.811341	0.001250	0.714279
-5.828021	-2.197093	3.821338	0.001220	0.714276
-5.739333	-2.124387	3.831334	0.001203	0.714452
-4.527017	-2.258608	3.841331	0.000978	0.714614
-4.968760	-2.181121	3.851328	0.001060	0.714612
-4.945924	-2.186479	3.861325	0.001056	0.714609
-4.356286	-2.176633	3.871322	0.000946	0.714837
-4.221977	-2.163889	3.881318	0.000921	0.714910
-4.256433	-2.156363	3.891315	0.000927	0.714912
-4.201105	-2.123479	3.901312	0.000917	0.714997
-3.921547	-2.052494	3.911309	0.000865	0.715237
-3.214143	-2.179925	3.921306	0.000734	0.715234
-3.235596	-2.172430	3.931302	0.000738	0.715241
-2.426504	-2.167039	3.941299	0.000587	0.715537
-2.359229	-2.169987	3.951296	0.000575	0.715555
-3.827967	-1.910383	3.961293	0.000848	0.715551
-2.254945	-2.035727	3.971290	0.000555	0.715858
-2.038623	-2.058637	3.981286	0.000515	0.715889
-2.897213	-1.890536	3.991283	0.000675	0.715919
-1.243633	-2.073106	4.001280	0.000367	0.716141
-2.109973	-1.920468	4.011277	0.000528	0.716137
-1.201386	-2.051260	4.021274	0.000359	0.716199
-1.991998	-1.781495	4.031270	0.000506	0.716454
-1.859348	-1.800498	4.041267	0.000482	0.716463
-1.605523	-1.694662	4.051264	0.000434	0.716762
-1.518491	-1.710432	4.061261	0.000418	0.716761
-1.275422	-1.588196	4.071258	0.000373	0.717089
-1.527063	-1.520056	4.081254	0.000420	0.717135
-1.031474	-1.481800	4.091251	0.000328	0.717385
-0.771248	-1.473204	4.101248	0.000279	0.717493
-0.707724	-1.376981	4.111245	0.000267	0.717706
-0.830945	-1.268425	4.121242	0.000290	0.717877
-0.816169	-1.196096	4.131238	0.000288	0.718025
-0.853477	-1.024298	4.141235	0.000294	0.718351
-0.821168	-0.947918	4.151232	0.000288	0.718513
-0.878690	-0.845107	4.161229	0.000299	0.718696
-0.499991	-0.777508	4.171226	0.000229	0.718962
-0.216855	-0.699414	4.181222	0.000176	0.719216
0.195696	-0.676068	4.191219	0.000099	0.719406
-0.213677	-0.485978	4.201216	0.000175	0.719637
-0.325536	-0.330911	4.211213	0.000196	0.719904
-0.231598	-0.198955	4.221210	0.000178	0.720196
-0.247183	-0.058310	4.231206	0.000181	0.720468
-0.021377	0.050162	4.241203	0.000139	0.720760
0.000000	0.189884	4.251200	0.000135	0.721043
0.324392	0.757281	4.256205	0.000074	0.722272
0.834484	1.934481	4.261210	-0.000021	0.724758
0.928813	3.779713	4.266214	-0.000040	0.728393
1.149166	6.157200	4.271219	-0.000083	0.733084
1.533917	9.009853	4.276224	-0.000156	0.738715
1.704693	12.380950	4.281229	-0.000190	0.745218
2.174207	16.148360	4.286234	-0.000280	0.752512
2.835424	20.295730	4.291238	-0.000406	0.760508
3.191140	24.895406	4.296243	-0.000475	0.769156
3.719482	29.833289	4.301248	-0.000576	0.778380
4.533664	35.077301	4.306253	-0.000731	0.788137
4.885085	40.713474	4.311258	-0.000800	0.798327
5.508821	46.608626	4.316262	-0.000920	0.808926
6.125774	52.784969	4.321267	-0.001039	0.819873
6.836154	59.223886	4.326272	-0.001176	0.831151
7.557128	65.893060	4.331277	-0.001314	0.842669
7.988849	72.826422	4.336282	-0.001399	0.854385
8.634196	79.936127	4.341286	-0.001524	0.866293
10.880490	86.959594	4.346291	-0.001947	0.878354
11.992142	94.381404	4.351296	-0.002159	0.890568
12.951601	101.991594	4.356301	-0.002342	0.902869
13.554661	109.810161	4.361306	-0.002460	0.915231
14.281640	117.725028	4.366310	-0.002600	0.927608
14.949854	125.766883	4.371315	-0.002730	0.939997
15.734160	133.890840	4.376320	-0.002881	0.952378
16.341413	142.134002	4.381325	-0.002999	0.964729
16.829545	150.472644	4.386330	-0.003096	0.977031
17.722130	158.834889	4.391334	-0.003267	0.989316
18.498064	167.254879	4.396339	-0.003417	1.001502
19.108642	175.750472	4.401344	-0.003536	1.013607
19.665750	184.288717	4.406349	-0.003646	1.025614
20.331688	192.841377	4.411354	-0.003775	1.037528
20.924919	201.431466	4.416358	-0.003891	1.049340
21.760944	209.993184	4.421363	-0.004053	1.061038
22.538155	218.602184	4.426368	-0.004203	1.072657
23.014921	227.265463	4.431373	-0.004297	1.084154
23.580116	235.913530	4.436378	-0.004408	1.095531
24.542028	244.504250	4.441382	-0.004593	1.106804
24.976350	253.195261	4.446387	-0.004679	1.117975
25.085914	261.919102	4.451392	-0.004705	1.129006
25.709737	270.570377	4.456397	-0.004827	1.139951
26.237411	279.231199	4.461402	-0.004931	1.150782
26.720041	287.888195	4.466406	-0.005026	1.161498
27.222753	296.507330	4.471411	-0.005126	1.172074
28.087655	305.053160	4.476416	-0.005292	1.182541
28.581643	313.676216	4.481421	-0.005390	1.192933
28.894013	322.288388	4.486426	-0.005454	1.203185
29.451515	330.870384	4.491430	-0.005563	1.213365
30.197500	339.398195	4.496435	-0.005707	1.223433
30.664130	347.987691	4.501440	-0.005800	1.233435
31.157383	356.534470	4.506445	-0.005897	1.243313
31.660194	365.063609	4.511450	-0.005996	1.253095
32.350591	373.555420	4.516454	-0.006130	1.262795
32.821343	382.078657	4.521459	-0.006224	1.272414
33.377221	390.554059	4.526464	-0.006333	1.281923
34.037087	399.029139	4.531469	-0.006461	1.291381
34.337869	407.527630	4.536474	-0.006522	1.300730
34.938701	416.024845	4.541478	-0.006640	1.310065
35.642874	424.505008	4.546483	-0.006776	1.319334
35.940522	432.947373	4.551488	-0.006837	1.328425
36.528239	441.351046	4.556493	-0.006952	1.337465
36.882491	449.757018	4.561498	-0.007024	1.346405
37.111365	458.208744	4.566502	-0.007072	1.355311
37.839613	466.525427	4.571507	-0.007213	1.364106
38.565975	474.861926	4.576512	-0.007353	1.372864
39.148046	483.234696	4.581517	-0.007467	1.381579
39.832208	491.574063	4.586522	-0.007600	1.390223
40.552265	499.915338	4.591526	-0.007740	1.398820
41.130363	508.237871	4.596531	-0.007853	1.407322
41.616320	516.587919	4.601536	-0.007948	1.415785
42.087190	524.938028	4.606541	-0.008042	1.424196
42.770907	533.243786	4.611546	-0.008174	1.432547
43.460019	541.539435	4.616550	-0.008308	1.440841
44.460876	549.793800	4.621555	-0.008500	1.449097
44.777733	558.156987	4.626560	-0.008564	1.457302
45.714524	566.417090	4.631565	-0.008744	1.465460
46.374807	574.760009	4.636570	-0.008872	1.473608
47.092478	583.027864	4.641574	-0.009011	1.481648
47.803206	591.279925	4.646579	-0.009149	1.489629
48.183964	599.597341	4.651584	-0.009225	1.497577
49.008992	607.826122	4.656589	-0.009384	1.505469
50.144079	616.023476	4.661594	-0.009601	1.513337
51.043923	624.248321	4.666598	-0.009774	1.521153
51.542449	632.555148	4.671603	-0.009872	1.528945
51.895964	640.866790	4.676608	-0.009943	1.536680
52.692378	649.096216	4.681613	-0.010097	1.544366
53.083156	657.399709	4.686618	-0.010175	1.552022
53.419767	665.680295	4.691622	-0.010243	1.559611
54.098535	673.882144	4.696627	-0.010375	1.567142
54.694684	682.116656	4.701632	-0.010491	1.574654
55.185439	690.363963	4.706637	-0.010588	1.582126
55.722721	698.588753	4.711642	-0.010693	1.589550
56.127586	706.853382	4.716646	-0.010774	1.596956
56.691785	715.052456	4.721651	-0.010884	1.604292
57.651517	723.212282	4.726656	-0.011068	1.611615
58.551757	731.400812	4.731661	-0.011241	1.618922
59.213200	739.591959	4.736666	-0.011370	1.626165
59.809456	747.884845	4.741670	-0.011486	1.633454
60.264505	756.088134	4.746675	-0.011576	1.640615
60.639062	764.299419	4.751680	-0.011651	1.647739
61.037439	772.529417	4.756685	-0.011731	1.654853
61.391079	780.729521	4.761690	-0.011802	1.661904
62.116508	788.889649	4.766694	-0.011942	1.668941
62.478996	797.113427	4.771699	-0.012015	1.675954
62.723986	805.311305	4.776704	-0.012066	1.682899
63.437088	813.466129	4.781709	-0.012204	1.689843
63.739222	821.679457	4.786714	-0.012266	1.696752
64.082953	829.872925	4.791718	-0.012335	1.703622
65.141146	837.975190	4.796723	-0.012537	1.710482
65.484664	846.192198	4.801728	-0.012607	1.717316
66.078586	854.349182	4.806733	-0.012722	1.724106
66.461351	862.520419	4.811738	-0.012799	1.730853
66.851843	870.710883	4.816742	-0.012877	1.737591
67.250329	878.889443	4.821747	-0.012957	1.744294
67.733490	887.044579	4.826752	-0.013052	1.750963
68.452170	895.187947	4.831757	-0.013191	1.757627
68.867513	903.338726	4.836762	-0.013274	1.764233
69.173635	911.534399	4.841766	-0.013336	1.770837
69.615897	919.711209	4.846771	-0.013423	1.777418
70.031251	927.854926	4.851776	-0.013506	1.783945
70.455274	936.055788	4.856781	-0.013590	1.790495
70.909578	944.237062	4.861786	-0.013680	1.797008
71.648171	952.319773	4.866790	-0.013823	1.803455
72.322254	960.422365	4.871795	-0.013954	1.809887
72.788734	968.562482	4.876800	-0.014046	1.816300
73.430227	976.685356	4.881805	-0.014171	1.822697
73.773053	984.843483	4.886810	-0.014240	1.829064
74.338316	992.986657	4.891814	-0.014350	1.835424
74.564206	1001.148636	4.896819	-0.014398	1.841736
74.945009	1009.289206	4.901824	-0.014474	1.848028
75.242513	1017.473120	4.906829	-0.014535	1.854321
75.701359	1025.584545	4.911834	-0.014625	1.860557
76.243200	1033.705387	4.916838	-0.014731	1.866789
76.707931	1041.877431	4.921843	-0.014823	1.873030
76.983704	1050.009012	4.926848	-0.014880	1.879198
77.723694	1058.085470	4.931853	-0.015023	1.885357
78.040738	1066.237072	4.936858	-0.015087	1.891504
78.288846	1074.400442	4.941862	-0.015139	1.897631
78.598732	1082.525447	4.946867	-0.015202	1.903718
79.090255	1090.626921	4.951872	-0.015298	1.909788
79.372276	1098.790543	4.956877	-0.015356	1.915861
79.831181	1106.873509	4.961882	-0.015447	1.921875
80.158708	1115.003528	4.966886	-0.015513	1.927890
80.588339	1123.140025	4.971891	-0.015598	1.933903
80.958768	1131.248896	4.976896	-0.015673	1.939870
81.234859	1139.390602	4.981901	-0.015729	1.945832
81.586214	1147.540864	4.986906	-0.015800	1.951790
81.844512	1155.683669	4.991910	-0.015853	1.957714
82.259689	1163.762070	4.996915	-0.015936	1.963591
83.193010	1171.775209	5.001920	-0.016115	1.969459
83.882060	1179.871526	5.006925	-0.016249	1.975343
84.164030	1187.993410	5.011930	-0.016306	1.981184
84.565656	1196.118638	5.016934	-0.016386	1.987023
85.125179	1204.232556	5.021939	-0.016496	1.992854
85.225388	1212.370377	5.026944	-0.016520	1.998635
85.682291	1220.458630	5.031949	-0.016610	2.004403
86.032588	1228.561091	5.036954	-0.016681	2.010153
86.532092	1236.669214	5.041958	-0.016779	2.015905
86.952196	1244.765830	5.046963	-0.016862	2.021625
87.597988	1252.837464	5.051968	-0.016988	2.027334
87.931655	1261.015155	5.056973	-0.017055	2.033069
88.356780	1269.091686	5.061978	-0.017140	2.038727
88.597983	1277.203154	5.066982	-0.017190	2.044375
88.977914	1285.310352	5.071987	-0.017266	2.050018
88.985322	1293.449904	5.076992	-0.017272	2.055630
89.515048	1301.527334	5.081997	-0.017376	2.061236
90.001777	1309.595178	5.087002	-0.017472	2.066817
90.331235	1317.725328	5.092006	-0.017539	2.072409
90.675063	1325.821756	5.097011	-0.017608	2.077964
91.316744	1333.848065	5.102016	-0.017733	2.083487
91.888324	1341.941634	5.107021	-0.017844	2.089033
92.206299	1350.060948	5.112026	-0.017909	2.094557
92.469575	1358.177690	5.117030	-0.017963	2.100059
92.921040	1366.247587	5.122035	-0.018052	2.105534
93.015064	1374.414278	5.127040	-0.018075	2.111024
93.510175	1382.527375	5.132045	-0.018173	2.116503
93.753013	1390.603692	5.137050	-0.018223	2.121919
93.908591	1398.704492	5.142054	-0.018257	2.127330
94.298997	1406.790638	5.147059	-0.018335	2.132739
94.711770	1414.844644	5.152064	-0.018417	2.138115
95.195045	1422.918836	5.157069	-0.018513	2.143497
95.461429	1431.004458	5.162074	-0.018568	2.148853
95.828932	1439.120014	5.167078	-0.018641	2.154225
96.299298	1447.182821	5.172083	-0.018734	2.159558
96.406696	1455.274694	5.177088	-0.018759	2.164863
96.621285	1463.396148	5.182093	-0.018804	2.170185
97.197955	1471.446620	5.187098	-0.018917	2.175481
97.261007	1479.549187	5.192102	-0.018934	2.180750
97.509150	1487.642511	5.197107	-0.018986	2.186017
98.046164	1495.688535	5.202112	-0.019091	2.191268
98.575380	1503.782753	5.207117	-0.019195	2.196536
98.905506	1511.832369	5.212122	-0.019261	2.201745
99.255987	1519.908658	5.217126	-0.019332	2.206960
99.677968	1528.000353	5.222131	-0.019416	2.212179
99.643235	1536.117970	5.227136	-0.019414	2.217362
100.120757	1544.194644	5.232141	-0.019508	2.222552
100.573111	1552.227719	5.237146	-0.019598	2.227699
101.042493	1560.326357	5.242150	-0.019691	2.232878
101.491142	1568.394450	5.247155	-0.019779	2.238024
101.490361	1576.504608	5.252160	-0.019784	2.243145
101.718309	1584.598934	5.257165	-0.019832	2.248264
102.005216	1592.685522	5.262170	-0.019891	2.253372
102.230349	1600.760640	5.267174	-0.019938	2.258455
102.743788	1608.818832	5.272179	-0.020039	2.263542
102.900791	1616.903400	5.277184	-0.020073	2.268602
103.166986	1625.063781	5.282189	-0.020128	2.273708
103.485567	1633.094146	5.287194	-0.020193	2.278726
103.881918	1641.126668	5.292198	-0.020272	2.283741
104.122927	1649.192241	5.297203	-0.020322	2.288753
104.289043	1657.272568	5.302208	-0.020358	2.293755
104.646029	1665.335288	5.307213	-0.020430	2.298753
104.716143	1673.409440	5.312218	-0.020448	2.303722
104.955956	1681.485718	5.317222	-0.020498	2.308696
105.459236	1689.551434	5.322227	-0.020597	2.313675
105.755282	1697.585174	5.327232	-0.020657	2.318606
105.927095	1705.673191	5.332237	-0.020694	2.323549
106.019167	1713.763223	5.337242	-0.020717	2.328477
106.490809	1721.820600	5.342246	-0.020810	2.333405
106.632449	1729.912075	5.347251	-0.020841	2.338317
106.730819	1737.984135	5.352256	-0.020865	2.343203
107.066794	1746.056205	5.357261	-0.020933	2.348098
107.451433	1754.135656	5.362266	-0.021010	2.352991
107.404283	1762.221076	5.367270	-0.021006	2.357843
107.904407	1770.251097	5.372275	-0.021104	2.362695
107.917134	1778.319497	5.377280	-0.021112	2.367522
108.278774	1786.394347	5.382285	-0.021185	2.372370
108.565724	1794.450092	5.387290	-0.021243	2.377191
109.027034	1802.471133	5.392294	-0.021334	2.381995
109.392372	1810.554206	5.397299	-0.021408	2.386819
109.648681	1818.621751	5.402304	-0.021461	2.391615
109.867118	1826.712318	5.407309	-0.021506	2.396413
110.014239	1834.763041	5.412314	-0.021539	2.401171
110.150842	1842.824603	5.417318	-0.021570	2.405925
110.445669	1850.905381	5.422323	-0.021630	2.410694
110.730753	1858.964468	5.427328	-0.021688	2.415440
111.018789	1867.022650	5.432333	-0.021747	2.420176
111.411918	1875.052924	5.437338	-0.021825	2.424895
111.930390	1883.106400	5.442342	-0.021927	2.429627
112.229878	1891.273890	5.447347	-0.021988	2.434400
112.425065	1899.289373	5.452352	-0.022030	2.439067
112.575681	1907.348058	5.457357	-0.022063	2.443746
112.671260	1915.405480	5.462362	-0.022086	2.448412
112.961512	1923.464438	5.467366	-0.022145	2.453085
113.430650	1931.488931	5.472371	-0.022238	2.457742
113.693659	1939.536086	5.477376	-0.022292	2.462388
114.093212	1947.594664	5.482381	-0.022372	2.467042
114.415709	1955.662681	5.487386	-0.022437	2.471686
114.579081	1963.743035	5.492390	-0.022473	2.476317
114.707509	1971.806752	5.497395	-0.022502	2.480928
114.862851	1979.855177	5.502400	-0.022536	2.485523
115.297500	1987.894205	5.507405	-0.022622	2.490124
115.669211	1995.962320	5.512410	-0.022697	2.494729
115.877332	2004.017628	5.517414	-0.022741	2.499306
116.112327	2012.085479	5.522419	-0.022790	2.503884
116.212337	2020.152976	5.527424	-0.022813	2.508444
116.507755	2028.274435	5.532429	-0.022874	2.513039
116.548794	2036.330253	5.537434	-0.022887	2.517571
116.676812	2044.363291	5.542438	-0.022916	2.522088
116.847133	2052.402332	5.547443	-0.022953	2.526604
116.972407	2060.467221	5.552448	-0.022981	2.531122
117.330094	2068.515245	5.557453	-0.023053	2.535640
117.580202	2076.535490	5.562458	-0.023105	2.540127
117.880482	2084.585039	5.567462	-0.023166	2.544625
118.202128	2092.649405	5.572467	-0.023231	2.549125
118.494275	2100.713368	5.577472	-0.023291	2.553615
118.789152	2108.779788	5.582477	-0.023351	2.558098
118.853506	2116.824937	5.587482	-0.023368	2.562546
119.312517	2124.830846	5.592486	-0.023459	2.566991
119.553170	2132.936666	5.597491	-0.023509	2.571469
119.667695	2141.003839	5.602496	-0.023535	2.575909
119.896148	2149.065838	5.607501	-0.023583	2.580346
120.205068	2157.079538	5.612506	-0.023646	2.584755
120.430439	2165.150177	5.617510	-0.023693	2.589182
120.656375	2173.396202	5.622515	-0.023740	2.593696
120.924624	2181.405630	5.627520	-0.023795	2.598077
121.168195	2189.411138	5.632525	-0.023846	2.602447
121.113853	2197.427657	5.637530	-0.023841	2.606795
121.360528	2205.448342	5.642534	-0.023892	2.611158
121.587645	2213.499178	5.647539	-0.023940	2.615529
121.754578	2221.514396	5.652544	-0.023976	2.619869
122.051234	2229.540281	5.657549	-0.024036	2.624217
122.193885	2237.591733	5.662554	-0.024068	2.628561
122.273675	2245.669007	5.667558	-0.024088	2.632907
122.625666	2253.708670	5.672563	-0.024159	2.637244
122.835613	2261.721222	5.677568	-0.024203	2.641550
123.141094	2269.759492	5.682573	-0.024265	2.645868
123.187504	2277.826473	5.687578	-0.024279	2.650179
123.316546	2285.900020	5.692582	-0.024309	2.654491
123.733961	2293.934206	5.697587	-0.024392	2.658793
123.785129	2301.985198	5.702592	-0.024406	2.663074
124.266884	2310.012614	5.707597	-0.024501	2.667363
124.872198	2318.034081	5.712602	-0.024619	2.671651
125.007712	2326.141227	5.717606	-0.024650	2.675946
125.390711	2334.161632	5.722611	-0.024726	2.680204
125.550717	2342.168669	5.727616	-0.024761	2.684435
125.806947	2350.243901	5.732621	-0.024814	2.688700
125.917887	2358.324672	5.737626	-0.024840	2.692953
125.910418	2366.399796	5.742630	-0.024844	2.697188
126.289257	2374.418474	5.747635	-0.024920	2.701411
126.416526	2382.456242	5.752640	-0.024948	2.705622
126.682096	2390.508582	5.757645	-0.025003	2.709843
126.914011	2398.592053	5.762650	-0.025052	2.714071
126.868404	2406.627790	5.767654	-0.025048	2.718251
127.057253	2414.665336	5.772659	-0.025089	2.722439
127.337438	2422.670171	5.777664	-0.025146	2.726610
127.549825	2430.734093	5.782669	-0.025191	2.730800
127.951639	2438.771731	5.787674	-0.025271	2.734983
128.030619	2446.818439	5.792678	-0.025291	2.739143
128.367272	2454.854209	5.797683	-0.025359	2.743308
128.655545	2462.887476	5.802688	-0.025417	2.747462
128.763053	2471.013344	5.807693	-0.025443	2.751646
129.121268	2479.093519	5.812698	-0.025515	2.755815
129.529163	2487.066924	5.817702	-0.025596	2.759927
129.648186	2495.110170	5.822707	-0.025623	2.764050
129.796718	2503.139422	5.827712	-0.025656	2.768162
130.056648	2511.201351	5.832717	-0.025710	2.772291
130.129258	2519.260537	5.837722	-0.025728	2.776402
130.437407	2527.266178	5.842726	-0.025791	2.780493
130.786967	2535.293116	5.847731	-0.025861	2.784591
130.736600	2543.360077	5.852736	-0.025857	2.788680
131.099084	2551.395899	5.857741	-0.025930	2.792771
131.343588	2559.441936	5.862746	-0.025981	2.796855
131.633796	2567.461184	5.867750	-0.026040	2.800922
131.875096	2575.505337	5.872755	-0.026090	2.804992
132.147885	2583.539075	5.877760	-0.026146	2.809053
132.346884	2591.629127	5.882765	-0.026188	2.813132
132.633994	2599.658072	5.887770	-0.026247	2.817180
132.878754	2607.690500	5.892774	-0.026298	2.821221
133.293274	2615.724521	5.897779	-0.026380	2.825267
133.480846	2623.763728	5.902784	-0.026420	2.829296
133.598004	2631.868225	5.907789	-0.026447	2.833349
133.749784	2639.905245	5.912794	-0.026481	2.837364
134.096607	2647.879477	5.917798	-0.026551	2.841353
134.154875	2655.930538	5.922803	-0.026567	2.845358
134.280925	2663.968311	5.927808	-0.026595	2.849355
134.531203	2672.033652	5.932813	-0.026647	2.853366
134.694648	2680.079897	5.937818	-0.026683	2.857358
134.760297	2688.110587	5.942822	-0.026700	2.861331
135.391678	2696.105928	5.947827	-0.026823	2.865313
135.710102	2704.136480	5.952832	-0.026888	2.869289
135.775515	2712.215602	5.957837	-0.026905	2.873269
136.057402	2720.265855	5.962842	-0.026963	2.877241
136.223542	2728.309138	5.967846	-0.026999	2.881199
136.356855	2736.337918	5.972851	-0.027029	2.885141
136.545598	2744.386908	5.977856	-0.027069	2.889092
136.893255	2752.440868	5.982861	-0.027139	2.893047
136.970998	2760.493112	5.987866	-0.027159	2.896982
136.997041	2768.529396	5.992870	-0.027169	2.900901
137.611204	2776.526313	5.997875	-0.027288	2.904828
137.809546	2784.568709	6.002880	-0.027331	2.908748
137.747773	2792.717000	6.007885	-0.027324	2.912701
138.117544	2800.759293	6.012890	-0.027398	2.916620
138.220959	2808.725709	6.017894	-0.027423	2.920483
138.495390	2816.731805	6.022899	-0.027479	2.924369
138.491548	2824.795960	6.027904	-0.027484	2.928263
138.880927	2832.831162	6.032909	-0.027561	2.932159
139.143351	2840.861912	6.037914	-0.027615	2.936040
139.378158	2848.867472	6.042918	-0.027664	2.939903
139.937236	2856.880346	6.047923	-0.027774	2.943781
139.957017	2864.931945	6.052928	-0.027783	2.947645
139.987233	2873.022341	6.057933	-0.027793	2.951522
140.297020	2881.054025	6.062938	-0.027856	2.955381
140.830751	2889.025814	6.067942	-0.027961	2.959218
140.967029	2897.056904	6.072947	-0.027991	2.963057
141.102999	2905.112290	6.077952	-0.028022	2.966903
141.625882	2913.155753	6.082957	-0.028125	2.970758
142.020760	2921.217735	6.087962	-0.028203	2.974610
142.126655	2929.242948	6.092966	-0.028228	2.978425
142.626462	2937.281312	6.097971	-0.028327	2.982262
142.764162	2945.314082	6.102976	-0.028357	2.986072
142.847111	2953.386792	6.107981	-0.028378	2.989894
143.013854	2961.456365	6.112986	-0.028414	2.993713
143.379958	2969.438404	6.117990	-0.028488	2.997497
143.557758	2977.496382	6.122995	-0.028526	3.001301
143.737731	2985.487433	6.128000	-0.028565	3.005070
144.053070	2993.530875	6.133005	-0.028629	3.008865
144.444592	3001.589954	6.138010	-0.028707	3.012666
144.660097	3009.631229	6.143014	-0.028752	3.016446
144.955372	3017.628977	6.148019	-0.028812	3.020204
145.171541	3025.667832	6.153024	-0.028858	3.023973
145.444876	3033.706191	6.158029	-0.028914	3.027740
145.530845	3041.788282	6.163034	-0.028935	3.031513
145.820034	3049.810417	6.168038	-0.028994	3.035263
146.200840	3057.832456	6.173043	-0.029070	3.039014
146.167124	3065.857767	6.178048	-0.029069	3.042741
146.551707	3073.881998	6.183053	-0.029146	3.046483
146.785936	3081.925741	6.188058	-0.029195	3.050222
146.592774	3090.007956	6.193062	-0.029164	3.053954
146.847749	3098.048516	6.198067	-0.029217	3.057683
147.169333	3106.040787	6.203072	-0.029282	3.061389
147.489345	3114.055267	6.208077	-0.029347	3.065101
147.596867	3122.121007	6.213082	-0.029372	3.068821
147.713214	3130.191624	6.218086	-0.029399	3.072540
148.141009	3138.268942	6.223091	-0.029484	3.076272
148.217741	3146.239491	6.228096	-0.029503	3.079933
148.408133	3154.262565	6.233101	-0.029544	3.083620
148.508698	3162.302387	6.238106	-0.029568	3.087306
148.746486	3170.313426	6.243110	-0.029617	3.090981
149.140520	3178.369670	6.248115	-0.029696	3.094679
149.294994	3186.385225	6.253120	-0.029730	3.098343
149.580760	3194.416365	6.258125	-0.029788	3.102015
149.697274	3202.446683	6.263130	-0.029815	3.105676
149.584221	3210.485451	6.268134	-0.029799	3.109325
149.882554	3218.575104	6.273139	-0.029860	3.113012
150.022482	3226.600056	6.278144	-0.029891	3.116657
150.329655	3234.581305	6.283149	-0.029954	3.120287
150.503234	3242.636355	6.288154	-0.029991	3.123939
150.814517	3250.611256	6.293158	-0.030054	3.127557
151.019771	3258.688385	6.298163	-0.030098	3.131213
151.303847	3266.719483	6.303168	-0.030156	3.134846
151.566801	3274.744788	6.308173	-0.030210	3.138472
151.871866	3282.767043	6.313178	-0.030272	3.142094
152.191464	3290.776432	6.318182	-0.030337	3.145707
152.301985	3298.857423	6.323187	-0.030363	3.149339
152.540857	3306.906695	6.328192	-0.030412	3.152957
152.486987	3314.971554	6.333197	-0.030408	3.156566
152.743235	3322.951893	6.338202	-0.030460	3.160146
153.031150	3330.948831	6.343206	-0.030519	3.163731
153.161400	3338.995469	6.348211	-0.030549	3.167328
153.374680	3347.010355	6.353216	-0.030594	3.170909
153.527978	3355.085111	6.358221	-0.030627	3.174511
153.879247	3363.106501	6.363226	-0.030698	3.178093
154.003766	3371.125164	6.368230	-0.030726	3.181660
154.400849	3379.163359	6.373235	-0.030806	3.185244
154.525780	3387.195278	6.378240	-0.030834	3.188809
154.714906	3395.258347	6.383245	-0.030874	3.192386
155.036109	3403.299604	6.388250	-0.030939	3.195955
155.232200	3411.281299	6.393254	-0.030981	3.199489
155.462741	3419.334493	6.398259	-0.031029	3.203052
155.691536	3427.332442	6.403264	-0.031077	3.206586
155.927719	3435.375535	6.408269	-0.031126	3.210137
155.999309	3443.460236	6.413274	-0.031145	3.213695
156.369166	3451.429137	6.418278	-0.031219	3.217211
156.823796	3459.478001	6.423283	-0.031309	3.220761
156.810449	3467.495763	6.428288	-0.031311	3.224275
156.884018	3475.557661	6.433293	-0.031330	3.227807
157.420720	3483.578753	6.438298	-0.031436	3.231337
157.617091	3491.649186	6.443302	-0.031477	3.234871
157.767946	3499.658330	6.448307	-0.031511	3.238372
157.911926	3507.663244	6.453312	-0.031543	3.241867
158.223222	3515.642010	6.458317	-0.031606	3.245353
158.524947	3523.682825	6.463322	-0.031667	3.248863
158.706414	3531.714823	6.468326	-0.031706	3.252360
159.012511	3539.801670	6.473331	-0.031768	3.255882
158.997762	3547.800803	6.478336	-0.031771	3.259349
159.061955	3555.854595	6.483341	-0.031788	3.262839
159.307692	3563.854959	6.488346	-0.031839	3.266310
159.489706	3571.869050	6.493350	-0.031878	3.269780
159.598673	3579.959909	6.498355	-0.031904	3.273277
159.766985	3588.007727	6.503360	-0.031940	3.276754
160.128353	3595.961838	6.508365	-0.032013	3.280195
160.246324	3603.998765	6.513370	-0.032040	3.283658
160.421271	3612.022384	6.518374	-0.032078	3.287114
160.816652	3620.071783	6.523379	-0.032156	3.290585
161.130153	3628.101557	6.528384	-0.032220	3.294042
161.142286	3636.156018	6.533389	-0.032227	3.297493
161.689346	3644.152086	6.538394	-0.032334	3.300937
161.557472	3652.164073	6.543398	-0.032315	3.304358
162.050204	3660.195199	6.548403	-0.032412	3.307807
162.048542	3668.284032	6.553408	-0.032417	3.311258
162.322026	3676.313665	6.558413	-0.032473	3.314691
162.578704	3684.335644	6.563418	-0.032526	3.318117
162.619861	3692.327799	6.568422	-0.032539	3.321518
162.987889	3700.314067	6.573427	-0.032613	3.324925
163.196363	3708.343345	6.578432	-0.032657	3.328341
163.447748	3716.402996	6.583437	-0.032709	3.331768
163.646060	3724.453598	6.588442	-0.032751	3.335186
163.872142	3732.471013	6.593446	-0.032798	3.338587
164.105949	3740.522645	6.598451	-0.032847	3.341999
164.605090	3748.481889	6.603456	-0.032945	3.345379
165.094560	3756.524307	6.608461	-0.033041	3.348790
165.609515	3764.572219	6.613466	-0.033143	3.352200
165.614880	3772.618433	6.618470	-0.033149	3.355588
166.362100	3780.586577	6.623475	-0.033293	3.358966
166.583834	3788.640999	6.628480	-0.033340	3.362358
166.701688	3796.673881	6.633485	-0.033367	3.365734
167.017770	3804.733682	6.638490	-0.033431	3.369125
167.301103	3812.756086	6.643494	-0.033489	3.372495
167.556776	3820.825590	6.648499	-0.033542	3.375881
167.532764	3828.825478	6.653504	-0.033542	3.379224
167.678057	3836.844355	6.658509	-0.033575	3.382578
167.933276	3844.875442	6.663514	-0.033627	3.385938
167.940040	3852.903383	6.668518	-0.033634	3.389284
168.502501	3861.004992	6.673523	-0.033744	3.392677
168.497448	3869.063548	6.678528	-0.033748	3.396029
168.588874	3877.012237	6.683533	-0.033770	3.399335
168.798978	3885.028763	6.688538	-0.033815	3.402670
168.767215	3893.023734	6.693542	-0.033814	3.405985
169.129758	3901.061508	6.698547	-0.033887	3.409328
169.288510	3909.123521	6.703552	-0.033921	3.412670
169.760269	3917.117728	6.708557	-0.034014	3.415992
169.992590	3925.141251	6.713562	-0.034063	3.419314
169.986378	3933.141656	6.718566	-0.034067	3.422616
170.271953	3941.163662	6.723571	-0.034125	3.425933
170.628826	3949.196832	6.728576	-0.034197	3.429254
171.444720	3957.188990	6.733581	-0.034354	3.432570
171.930479	3965.221556	6.738586	-0.034450	3.435889
172.498139	3973.199926	6.743590	-0.034560	3.439184
173.036830	3981.251767	6.748595	-0.034666	3.442506
173.329111	3989.273711	6.753600	-0.034726	3.445803
173.579167	3997.338938	6.758605	-0.034777	3.449114
173.704498	4005.413706	6.763610	-0.034806	3.452422
173.799979	4013.446717	6.768614	-0.034829	3.455708
174.272048	4021.483189	6.773619	-0.034922	3.459005
174.561580	4029.478626	6.778624	-0.034981	3.462276
174.653164	4037.498353	6.783629	-0.035003	3.465547
174.760638	4045.585048	6.788634	-0.035029	3.468843
175.014117	4053.604141	6.793638	-0.035081	3.472113
175.289064	4061.646125	6.798643	-0.035138	3.475390
175.474446	4069.629834	6.803648	-0.035177	3.478637
176.734392	4077.550116	6.808653	-0.035417	3.481890
177.388400	4085.573911	6.813658	-0.035544	3.485162
177.888053	4093.603796	6.818662	-0.035642	3.488428
178.512619	4101.682632	6.823667	-0.035764	3.491716
178.879139	4109.706834	6.828672	-0.035837	3.494969
179.089664	4117.733830	6.833677	-0.035882	3.498216
179.104931	4125.809905	6.838682	-0.035890	3.501474
179.377706	4133.746405	6.843686	-0.035946	3.504680
179.934642	4141.821173	6.848691	-0.036055	3.507948
179.998556	4149.875774	6.853696	-0.036072	3.511189
180.175957	4157.898021	6.858701	-0.036110	3.514418
180.426577	4165.955570	6.863706	-0.036162	3.517660
180.369712	4173.932860	6.868710	-0.036156	3.520858
180.682563	4181.949934	6.873715	-0.036220	3.524079
180.822066	4189.991609	6.878720	-0.036251	3.527303
181.243569	4198.017712	6.883725	-0.036335	3.530526
181.348672	4206.078467	6.888730	-0.036359	3.533750
181.561309	4214.082174	6.893734	-0.036404	3.536951
181.894475	4222.084928	6.898739	-0.036471	3.540153
181.903022	4230.131268	6.903744	-0.036478	3.543360
182.200245	4238.156184	6.908749	-0.036539	3.546564
182.500000	4246.183598	6.913754	-0.036600	3.549766
182.436043	4254.308433	6.918758	-0.036593	3.552993
182.663807	4262.365418	6.923763	-0.036641	3.556198
183.041978	4270.283184	6.928768	-0.036716	3.559350
183.065100	4278.285670	6.933773	-0.036726	3.562523
183.232715	4286.319339	6.938778	-0.036762	3.565709
183.568270	4294.313164	6.943782	-0.036830	3.568881
184.009706	4302.359425	6.948787	-0.036917	3.572074
184.040504	4310.395734	6.953792	-0.036928	3.575248
184.213997	4318.404235	6.958797	-0.036966	3.578413
184.441285	4326.465908	6.963802	-0.037013	3.581598
184.561498	4334.423694	6.968806	-0.037041	3.584735
184.788280	4342.487941	6.973811	-0.037088	3.587915
185.102695	4350.488764	6.978816	-0.037152	3.591070
185.281830	4358.520841	6.983821	-0.037191	3.594230
185.513223	4366.547561	6.988826	-0.037239	3.597386
185.646757	4374.539077	6.993830	-0.037269	3.600524
185.995864	4382.553301	6.998835	-0.037339	3.603673
185.941713	4390.589905	7.003840	-0.037334	3.606817
185.970046	4398.626837	7.008845	-0.037345	3.609961
186.457708	4406.673376	7.013850	-0.037441	3.613119
186.402326	4414.713602	7.018854	-0.037436	3.616256
186.866793	4422.684072	7.023859	-0.037527	3.619378
187.146112	4430.704322	7.028864	-0.037585	3.622511
187.329744	4438.727935	7.033869	-0.037624	3.625640
187.681295	4446.784553	7.038874	-0.037695	3.628784
187.835037	4454.818735	7.043878	-0.037729	3.631911
188.323095	4462.868020	7.048883	-0.037825	3.635050
188.379300	4470.868326	7.053888	-0.037840	3.638156
188.589340	4478.884192	7.058893	-0.037885	3.641269
188.779707	4486.869672	7.063898	-0.037925	3.644367
189.122772	4494.888656	7.068902	-0.037994	3.647480
189.563269	4502.929774	7.073907	-0.038082	3.650601
189.690728	4510.976760	7.078912	-0.038111	3.653713
189.753414	4519.022954	7.083917	-0.038127	3.656821
189.774376	4527.051333	7.088922	-0.038137	3.659918
189.848188	4535.062681	7.093926	-0.038155	3.663007
190.396509	4543.102275	7.098931	-0.038263	3.666117
190.522729	4551.102724	7.103936	-0.038291	3.669198
190.633371	4559.149198	7.108941	-0.038317	3.672294
191.035556	4567.170771	7.113946	-0.038397	3.675385
191.301288	4575.143291	7.118950	-0.038452	3.678451
191.377514	4583.232161	7.123955	-0.038471	3.681555
191.512463	4591.167455	7.128960	-0.038502	3.684598
191.847949	4599.225828	7.133965	-0.038569	3.687691
192.127961	4607.272738	7.138970	-0.038627	3.690775
192.503254	4615.260566	7.143974	-0.038702	3.693837
192.935163	4623.315285	7.148979	-0.038787	3.696923
192.982579	4631.326791	7.153984	-0.038802	3.699981
193.035096	4639.340521	7.158989	-0.038816	3.703036
193.354218	4647.381268	7.163994	-0.038881	3.706107
193.646676	4655.371466	7.168998	-0.038941	3.709154
193.826722	4663.453686	7.174003	-0.038980	3.712232
194.023638	4671.529280	7.179008	-0.039021	3.715304
194.563118	4679.490056	7.184013	-0.039127	3.718339
194.510523	4687.535077	7.189018	-0.039122	3.721389
194.624985	4695.463088	7.194022	-0.039149	3.724396
194.898586	4703.507849	7.199027	-0.039205	3.727449
195.148796	4711.540180	7.204032	-0.039257	3.730494
194.966632	4719.582622	7.209037	-0.039228	3.733530
195.272530	4727.655289	7.214042	-0.039290	3.736586
195.721774	4735.570098	7.219046	-0.039379	3.739584
195.658403	4743.636278	7.224051	-0.039373	3.742624
195.853952	4751.638086	7.229056	-0.039414	3.745644
196.026075	4759.648735	7.234061	-0.039451	3.748664
196.528286	4767.730089	7.239066	-0.039550	3.751715
196.496753	4775.741650	7.244070	-0.039550	3.754726
196.824593	4783.746577	7.249075	-0.039616	3.757740
197.113303	4791.774640	7.254080	-0.039675	3.760759
196.937527	4799.788665	7.259085	-0.039647	3.763760
197.272255	4807.872802	7.264090	-0.039715	3.766796
197.492151	4815.842140	7.269094	-0.039761	3.769785
197.548724	4823.894635	7.274099	-0.039777	3.772798
197.532890	4831.949633	7.279104	-0.039779	3.775808
197.820208	4839.930018	7.284109	-0.039838	3.778795
198.254769	4847.986655	7.289114	-0.039924	3.781811
198.337844	4855.948728	7.294118	-0.039944	3.784782
198.525761	4863.990465	7.299123	-0.039985	3.787782
198.945101	4872.017312	7.304128	-0.040068	3.790780
199.136701	4880.058365	7.309133	-0.040109	3.793775
199.245469	4888.130939	7.314138	-0.040134	3.796778
199.312396	4896.043393	7.319142	-0.040152	3.799718
199.491468	4904.093437	7.324147	-0.040190	3.802709
199.654227	4912.088531	7.329152	-0.040226	3.805677
199.761239	4920.101634	7.334157	-0.040251	3.808648
200.156996	4928.144712	7.339162	-0.040330	3.811634
200.297069	4936.161849	7.344166	-0.040361	3.814603
200.477823	4944.206604	7.349171	-0.040400	3.817581
200.869087	4952.182157	7.354176	-0.040478	3.820535
200.916243	4960.193156	7.359181	-0.040492	3.823492
201.131206	4968.276993	7.364186	-0.040537	3.826478
201.031878	4976.275854	7.369190	-0.040524	3.829423
201.470401	4984.312145	7.374195	-0.040611	3.832391
201.615190	4992.329080	7.379200	-0.040643	3.835343
201.647960	5000.329709	7.384205	-0.040654	3.838285
202.185147	5008.339538	7.389210	-0.040760	3.841239
202.252736	5016.358311	7.394214	-0.040777	3.844183
202.444992	5024.380551	7.399219	-0.040818	3.847130
202.671965	5032.390052	7.404224	-0.040866	3.850070
203.020670	5040.444219	7.409229	-0.040936	3.853026
203.291761	5048.487689	7.414234	-0.040992	3.855975
203.471985	5056.511703	7.419238	-0.041030	3.858912
203.885147	5064.525692	7.424243	-0.041113	3.861849
203.852031	5072.529346	7.429248	-0.041112	3.864770
204.228523	5080.556075	7.434253	-0.041187	3.867706
204.480482	5088.594131	7.439258	-0.041239	3.870641
204.630188	5096.812009	7.444262	-0.041272	3.873637
204.669635	5104.850912	7.449267	-0.041285	3.876563
205.122084	5112.718257	7.454272	-0.041374	3.879433
205.375614	5120.707998	7.459277	-0.041426	3.882342
205.319648	5128.720377	7.464282	-0.041421	3.885250
205.567230	5136.702792	7.469286	-0.041473	3.888152
205.836124	5144.726330	7.474291	-0.041528	3.891066
205.963875	5152.794495	7.479296	-0.041557	3.893992
206.110250	5160.815187	7.484301	-0.041589	3.896898
206.426579	5168.774320	7.489306	-0.041653	3.899783
206.671370	5176.805432	7.494310	-0.041704	3.902691
206.879882	5184.812543	7.499315	-0.041748	3.905588
206.982948	5192.856254	7.504320	-0.041773	3.908493
207.291693	5200.856411	7.509325	-0.041835	3.911384
207.592348	5208.926302	7.514330	-0.041896	3.914298
207.483726	5216.941808	7.519334	-0.041881	3.917183
208.070270	5224.895569	7.524339	-0.041996	3.920056
208.123925	5232.954619	7.529344	-0.042011	3.922955
208.415150	5240.926791	7.534349	-0.042070	3.925825
208.619928	5248.964088	7.539354	-0.042114	3.928715
208.718641	5256.997935	7.544358	-0.042137	3.931600
208.788221	5265.061837	7.549363	-0.042156	3.934492
209.156132	5273.051446	7.554368	-0.042229	3.937361
209.525803	5281.039979	7.559373	-0.042303	3.940228
209.728161	5289.087301	7.564378	-0.042346	3.943110
209.805112	5297.081268	7.569382	-0.042366	3.945969
210.156162	5305.101704	7.574387	-0.042436	3.948841
210.411739	5313.168677	7.579392	-0.042489	3.951725
210.596607	5321.202203	7.584397	-0.042529	3.954594
210.803821	5329.228298	7.589402	-0.042572	3.957458
210.918369	5337.172715	7.594406	-0.042599	3.960290
210.946744	5345.216523	7.599411	-0.042609	3.963153
211.218257	5353.229044	7.604416	-0.042665	3.966008
211.316398	5361.224105	7.609421	-0.042689	3.968851
211.580488	5369.306751	7.614426	-0.042743	3.971726
211.720773	5377.319396	7.619430	-0.042774	3.974572
212.202681	5385.348154	7.624435	-0.042869	3.977427
212.155854	5393.361906	7.629440	-0.042866	3.980267
212.295269	5401.349724	7.634445	-0.042897	3.983098
212.470886	5409.413974	7.639450	-0.042935	3.985954
212.525663	5417.399611	7.644454	-0.042950	3.988779
212.854672	5425.425996	7.649459	-0.043017	3.991621
213.172944	5433.477314	7.654464	-0.043081	3.994469
213.475293	5441.497191	7.659469	-0.043143	3.997304
213.606956	5449.503225	7.664474	-0.043172	4.000129
213.856709	5457.520254	7.669478	-0.043224	4.002958
214.257670	5465.539776	7.674483	-0.043304	4.005788
214.380186	5473.591886	7.679488	-0.043332	4.008623
214.434325	5481.598638	7.684493	-0.043347	4.011439
214.624443	5489.662753	7.689498	-0.043388	4.014275
214.617699	5497.676474	7.694502	-0.043392	4.017089
214.853689	5505.636120	7.699507	-0.043441	4.019885
215.094462	5513.681371	7.704512	-0.043491	4.022710
215.114871	5521.676979	7.709517	-0.043500	4.025511
215.400728	5529.737943	7.714522	-0.043558	4.028338
215.639824	5537.746030	7.719526	-0.043608	4.031143
215.922180	5545.886562	7.724531	-0.043666	4.033994
216.178454	5553.889289	7.729536	-0.043719	4.036794
216.206471	5561.769718	7.734541	-0.043729	4.039545
216.381154	5569.827411	7.739546	-0.043767	4.042359
216.530858	5577.798699	7.744550	-0.043800	4.045141
216.586512	5585.836892	7.749555	-0.043816	4.047942
216.711550	5593.841880	7.754560	-0.043844	4.050731
216.906462	5601.883627	7.759565	-0.043886	4.053532
217.039200	5609.941702	7.764570	-0.043916	4.056335
217.297175	5617.907629	7.769574	-0.043969	4.059106
217.450525	5625.930214	7.774579	-0.044002	4.061894
217.774343	5633.886559	7.779584	-0.044068	4.064659
217.784075	5641.945994	7.784589	-0.044075	4.067454
218.035414	5650.003842	7.789594	-0.044127	4.070249
218.209416	5658.009143	7.794598	-0.044165	4.073023
218.426016	5666.037218	7.799603	-0.044210	4.075804
218.600567	5674.020173	7.804608	-0.044248	4.078567
218.804532	5682.012869	7.809613	-0.044291	4.081331
219.021753	5690.020497	7.814618	-0.044337	4.084099
219.095521	5698.055625	7.819622	-0.044356	4.086873
219.151483	5706.058005	7.824627	-0.044371	4.089633
219.468217	5714.159830	7.829632	-0.044435	4.092429
219.666918	5722.136803	7.834637	-0.044478	4.095179
220.000049	5730.172094	7.839642	-0.044545	4.097948
220.301028	5738.164259	7.844646	-0.044606	4.100701
220.528167	5746.167488	7.849651	-0.044654	4.103454
220.607737	5754.236398	7.854656	-0.044674	4.106226
220.790139	5762.259569	7.859661	-0.044713	4.108982
220.819241	5770.301293	7.864666	-0.044723	4.111740
221.093611	5778.313692	7.869670	-0.044780	4.114490
221.420630	5786.373372	7.874675	-0.044846	4.117254
221.582950	5794.310608	7.879680	-0.044881	4.119973
221.737556	5802.348409	7.884685	-0.044915	4.122724
222.253823	5810.350912	7.889690	-0.045016	4.125466
222.422195	5818.347938	7.894694	-0.045053	4.128199
222.462808	5826.387023	7.899699	-0.045066	4.130944
222.927862	5834.448132	7.904704	-0.045158	4.133699
223.153979	5842.466635	7.909709	-0.045205	4.136435
223.456168	5850.472233	7.914714	-0.045266	4.139166
223.596733	5858.487182	7.919718	-0.045298	4.141896
223.764720	5866.467038	7.924723	-0.045334	4.144613
224.445111	5874.516800	7.929728	-0.045466	4.147358
224.546882	5882.507919	7.934733	-0.045490	4.150074
224.798855	5890.571748	7.939738	-0.045542	4.152815
225.243158	5898.640786	7.944742	-0.045630	4.155558
225.268935	5906.622022	7.949747	-0.045640	4.158264
225.452897	5914.626090	7.954752	-0.045680	4.160979
225.813710	5922.566719	7.959757	-0.045752	4.163672
226.124723	5930.678608	7.964762	-0.045815	4.166420
226.147099	5938.673662	7.969766	-0.045825	4.169124
226.390277	5946.705333	7.974771	-0.045875	4.171841
226.702297	5954.753923	7.979776	-0.045938	4.174563
226.965751	5962.726232	7.984781	-0.045993	4.177257
227.236459	5970.736897	7.989786	-0.046048	4.179962
227.373586	5978.760949	7.994790	-0.046079	4.182668
227.630025	5986.746511	7.999795	-0.046132	4.185361
228.281825	5994.806177	8.004800	-0.046258	4.188081
228.470579	6002.818481	8.009805	-0.046299	4.190778
228.824695	6010.920856	8.014810	-0.046370	4.193506
229.190339	6018.948351	8.019814	-0.046443	4.196207
229.283980	6026.874421	8.024819	-0.046466	4.198869
229.522026	6034.920174	8.029824	-0.046515	4.201571
229.564496	6042.870202	8.034829	-0.046529	4.204237
229.852508	6050.907160	8.039834	-0.046587	4.206933
230.055051	6058.901673	8.044838	-0.046630	4.209613
230.440874	6066.934954	8.049843	-0.046707	4.212305
230.817867	6074.968206	8.054848	-0.046783	4.214996
230.997309	6082.976280	8.059853	-0.046821	4.217674
231.247973	6090.957467	8.064858	-0.046873	4.220342
231.403853	6099.005583	8.069862	-0.046907	4.223030
231.539897	6106.987400	8.074867	-0.046938	4.225694
231.717111	6115.063036	8.079872	-0.046976	4.228388
231.909730	6123.033778	8.084877	-0.047017	4.231046
232.183396	6131.127324	8.089882	-0.047073	4.233743
232.425381	6139.133207	8.094886	-0.047124	4.236409
232.470844	6147.118878	8.099891	-0.047137	4.239065
232.799374	6155.166371	8.104896	-0.047204	4.241743
233.017990	6163.112175	8.109901	-0.047250	4.244384
233.377649	6171.180448	8.114906	-0.047322	4.247065
233.290341	6179.143086	8.119910	-0.047311	4.249705
233.456614	6187.238357	8.124915	-0.047347	4.252390
233.929070	6195.250273	8.129920	-0.047440	4.255048
234.076087	6203.285711	8.134925	-0.047473	4.257710
234.380529	6211.261569	8.139930	-0.047534	4.260351
234.437417	6219.269000	8.144934	-0.047550	4.262999
234.603112	6227.297438	8.149939	-0.047586	4.265654
234.757160	6235.382328	8.154944	-0.047620	4.268325
235.045491	6243.335391	8.159949	-0.047679	4.270952
235.506190	6251.435744	8.164954	-0.047770	4.273628
235.487284	6259.428728	8.169958	-0.047772	4.276262
235.660927	6267.409363	8.174963	-0.047809	4.278892
235.703115	6275.447672	8.179968	-0.047822	4.281539
236.051692	6283.411074	8.184973	-0.047892	4.284162
236.226726	6291.480751	8.189978	-0.047930	4.286816
236.460994	6299.460888	8.194982	-0.047979	4.289440
236.482105	6307.517861	8.199987	-0.047988	4.292086
236.776070	6315.530300	8.204992	-0.048048	4.294718
236.882241	6323.559020	8.209997	-0.048073	4.297352
237.037780	6331.540072	8.215002	-0.048107	4.299969
237.024376	6339.593029	8.220006	-0.048110	4.302607
237.260300	6347.563915	8.225011	-0.048159	4.305218
237.380229	6355.614069	8.230016	-0.048187	4.307853
237.708234	6363.624226	8.235021	-0.048253	4.310475
237.679974	6371.692580	8.240026	-0.048253	4.313111
237.797301	6379.685058	8.245030	-0.048280	4.315722
238.349093	6387.672524	8.250035	-0.048388	4.318333
238.521079	6395.685130	8.255040	-0.048425	4.320947
238.297166	6403.709622	8.260045	-0.048389	4.323561
238.770367	6411.748325	8.265050	-0.048482	4.326184
238.941247	6419.724900	8.270054	-0.048519	4.328782
239.020857	6427.789919	8.275059	-0.048539	4.331406
239.311780	6435.803438	8.280064	-0.048598	4.334014
239.554883	6443.819089	8.285069	-0.048649	4.336621
239.781874	6451.782316	8.290074	-0.048696	4.339209
239.869324	6459.838001	8.295078	-0.048718	4.341824
240.245973	6467.775101	8.300083	-0.048793	4.344401
240.396849	6475.905731	8.305088	-0.048826	4.347038
240.412440	6483.870631	8.310093	-0.048834	4.349619
240.545357	6491.915055	8.315098	-0.048864	4.352224
240.814394	6500.043660	8.320102	-0.048920	4.354856
241.068834	6507.986390	8.325107	-0.048972	4.357427
241.291298	6515.955805	8.330112	-0.049019	4.360004
241.287465	6523.923806	8.335117	-0.049023	4.362578
241.366918	6531.988748	8.340122	-0.049043	4.365182
241.638745	6539.993889	8.345126	-0.049099	4.367766
241.886869	6547.959784	8.350131	-0.049150	4.370336
242.243131	6556.003073	8.355136	-0.049222	4.372930
242.431929	6564.025297	8.360141	-0.049262	4.375515
242.773421	6572.059255	8.365146	-0.049331	4.378103
242.807430	6580.046401	8.370150	-0.049343	4.380672
242.981356	6588.043522	8.375155	-0.049380	4.383244
243.270519	6596.095860	8.380160	-0.049439	4.385833
243.412929	6604.077847	8.385165	-0.049471	4.388397
243.595140	6612.155353	8.390170	-0.049510	4.390990
243.529703	6620.194247	8.395174	-0.049503	4.393568
243.855264	6628.221473	8.400179	-0.049569	4.396142
244.080965	6636.224019	8.405184	-0.049616	4.398707
244.158263	6644.208430	8.410189	-0.049636	4.401264
244.516491	6652.206587	8.415194	-0.049708	4.403825
244.732982	6660.220632	8.420198	-0.049753	4.406388
244.707210	6668.221811	8.425203	-0.049754	4.408945
244.802515	6676.308830	8.430208	-0.049777	4.411529
244.983176	6684.342562	8.435213	-0.049815	4.414094
245.307292	6692.371008	8.440218	-0.049881	4.416657
245.349681	6700.351726	8.445222	-0.049894	4.419202
245.704445	6708.381384	8.450227	-0.049965	4.421762
246.151949	6716.411529	8.455232	-0.050054	4.424321
246.037372	6724.395853	8.460237	-0.050038	4.426862
246.286387	6732.436425	8.465242	-0.050089	4.429421
246.735576	6740.449436	8.470246	-0.050178	4.431970
246.854739	6748.501364	8.475251	-0.050206	4.434529
246.865581	6756.550645	8.480256	-0.050213	4.437085
247.099640	6764.470656	8.485261	-0.050262	4.439600
247.542724	6772.513555	8.490266	-0.050349	4.442153
247.518195	6780.473867	8.495270	-0.050350	4.444676
247.848328	6788.505043	8.500275	-0.050417	4.447221
248.002036	6796.537311	8.505280	-0.050450	4.449765
248.160465	6804.553459	8.510285	-0.050485	4.452302
248.308699	6812.607951	8.515290	-0.050518	4.454850
248.545088	6820.610710	8.520294	-0.050567	4.457381
248.777541	6828.600370	8.525299	-0.050616	4.459905
249.088077	6836.631317	8.530304	-0.050679	4.462442
249.256686	6844.613198	8.535309	-0.050715	4.464961
249.295244	6852.685331	8.540314	-0.050728	4.467507
249.362165	6860.708264	8.545318	-0.050745	4.470036
249.548176	6868.710658	8.550323	-0.050785	4.472557
250.072771	6876.743715	8.555328	-0.050888	4.475088
249.943837	6884.727990	8.560333	-0.050869	4.477599
250.202476	6892.713621	8.565338	-0.050922	4.480111
250.466288	6900.763410	8.570343	-0.050977	4.482642
250.577738	6908.720974	8.575347	-0.051003	4.485142
250.796547	6916.821235	8.580352	-0.051049	4.487685
250.847227	6924.798424	8.585357	-0.051063	4.490188
251.168074	6932.855197	8.590362	-0.051128	4.492716
251.300780	6940.862595	8.595367	-0.051158	4.495225
251.278906	6948.887908	8.600371	-0.051159	4.497739
251.785722	6956.866084	8.605376	-0.051259	4.500238
251.894275	6964.910287	8.610381	-0.051284	4.502755
252.014604	6972.891025	8.615386	-0.051312	4.505250
252.319914	6980.970629	8.620391	-0.051374	4.507776
252.321871	6988.931389	8.625395	-0.051379	4.510262
252.545540	6997.027838	8.630400	-0.051426	4.512790
252.968098	7004.992239	8.635405	-0.051510	4.515276
253.266788	7012.987181	8.640410	-0.051571	4.517770
253.455488	7020.932363	8.645415	-0.051611	4.520246
253.653426	7028.985192	8.650419	-0.051653	4.522755
254.029507	7037.002202	8.655424	-0.051729	4.525251
253.950939	7045.012840	8.660429	-0.051719	4.527743
254.218575	7053.032607	8.665434	-0.051774	4.530237
254.554831	7061.095657	8.670439	-0.051842	4.532743
254.700761	7069.075009	8.675443	-0.051874	4.535222
254.749620	7077.130804	8.680448	-0.051889	4.537723
255.182242	7085.079111	8.685453	-0.051974	4.540189
255.514626	7093.170463	8.690458	-0.052042	4.542699
255.599066	7101.142822	8.695463	-0.052062	4.545170
255.623308	7109.166255	8.700467	-0.052072	4.547655
256.063557	7117.180894	8.705472	-0.052159	4.550136
256.173276	7125.213808	8.710477	-0.052185	4.552622
256.340327	7133.258975	8.715482	-0.052221	4.555110
256.486850	7141.278391	8.720487	-0.052254	4.557588
256.706483	7149.210931	8.725491	-0.052300	4.560039
257.020453	7157.226349	8.730496	-0.052364	4.562514
256.982597	7165.229399	8.735501	-0.052362	4.564983
257.483921	7173.257064	8.740506	-0.052460	4.567459
257.622406	7181.319942	8.745511	-0.052491	4.569944
257.703184	7189.335757	8.750515	-0.052511	4.572413
258.228724	7197.413398	8.755520	-0.052615	4.574900
258.405999	7205.381974	8.760525	-0.052653	4.577352
258.412705	7213.377703	8.765530	-0.052659	4.579811
258.705447	7221.455254	8.770535	-0.052719	4.582294
258.772232	7229.427025	8.775539	-0.052737	4.584743
258.906803	7237.500592	8.780544	-0.052767	4.587222
259.038854	7245.410674	8.785549	-0.052797	4.589649
259.379688	7253.490610	8.790554	-0.052865	4.592128
259.410691	7261.498102	8.795559	-0.052876	4.594582
259.534831	7269.535254	8.800563	-0.052905	4.597044
259.807644	7277.513367	8.805568	-0.052960	4.599487
259.933888	7285.548018	8.810573	-0.052989	4.601946
260.196785	7293.484821	8.815578	-0.053043	4.604374
260.302780	7301.586391	8.820583	-0.053068	4.606851
260.492723	7309.513475	8.825587	-0.053109	4.609273
260.680423	7317.609452	8.830592	-0.053149	4.611745
260.740007	7325.640277	8.835597	-0.053165	4.614196
261.124966	7333.680590	8.840602	-0.053242	4.616649
261.377056	7341.636171	8.845607	-0.053294	4.619074
261.319566	7349.679888	8.850611	-0.053289	4.621525
261.493252	7357.670624	8.855616	-0.053326	4.623959
261.834301	7365.674018	8.860621	-0.053395	4.626395
262.028209	7373.725734	8.865626	-0.053436	4.628845
262.106207	7381.749801	8.870631	-0.053456	4.631284
262.543123	7389.743766	8.875635	-0.053543	4.633714
262.820207	7397.796310	8.880640	-0.053599	4.636159
262.856761	7405.760170	8.885645	-0.053611	4.638577
263.089683	7413.802733	8.890650	-0.053660	4.641017
263.485639	7421.815000	8.895655	-0.053739	4.643447
263.601764	7429.791760	8.900659	-0.053766	4.645864
263.567798	7437.836227	8.905664	-0.053765	4.648301
263.898083	7445.838538	8.910669	-0.053831	4.650724
264.213272	7453.910122	8.915674	-0.053895	4.653166
264.436258	7461.894912	8.920679	-0.053942	4.655581
264.532591	7469.875232	8.925683	-0.053965	4.657994
264.699120	7477.919940	8.930688	-0.054001	4.660424
264.593381	7485.908911	8.935693	-0.053987	4.662837
264.852185	7493.892103	8.940698	-0.054040	4.665246
265.178804	7502.028888	8.945703	-0.054106	4.667700
265.216224	7509.977179	8.950707	-0.054118	4.670097
265.532454	7518.028292	8.955712	-0.054182	4.672523
265.951920	7526.104962	8.960717	-0.054266	4.674955
266.284673	7534.128513	8.965722	-0.054333	4.677370
266.266665	7542.037211	8.970727	-0.054335	4.679749
266.374228	7550.027466	8.975731	-0.054360	4.682152
266.624499	7558.023723	8.980736	-0.054412	4.684555
266.609250	7566.087081	8.985741	-0.054414	4.686977
266.909905	7574.022362	8.990746	-0.054475	4.689359
267.216487	7582.112723	8.995751	-0.054538	4.691787
267.332394	7590.129127	9.000755	-0.054564	4.694191
267.557368	7598.152501	9.005760	-0.054611	4.696596
267.698508	7606.055486	9.010765	-0.054643	4.698963
267.972267	7614.144888	9.015770	-0.054699	4.701386
268.182331	7622.139004	9.020775	-0.054743	4.703778
268.354273	7630.171440	9.025779	-0.054781	4.706181
268.625460	7638.254765	9.030784	-0.054836	4.708597
268.569365	7646.214408	9.035789	-0.054831	4.710976
268.718727	7654.230932	9.040794	-0.054864	4.713370
269.197276	7662.283587	9.045799	-0.054958	4.715773
269.353702	7670.265626	9.050803	-0.054993	4.718155
269.588444	7678.252439	9.055808	-0.055042	4.720536
269.646643	7686.312019	9.060813	-0.055058	4.722939
269.711229	7694.290893	9.065818	-0.055075	4.725316
269.936608	7702.340309	9.070823	-0.055122	4.727712
269.883616	7710.364015	9.075827	-0.055117	4.730100
270.319619	7718.401694	9.080832	-0.055204	4.732490
270.482136	7726.387377	9.085837	-0.055239	4.734864
270.614683	7734.477715	9.090842	-0.055269	4.737268
270.736768	7742.413365	9.095847	-0.055297	4.739625
270.921467	7750.446231	9.100851	-0.055337	4.742009
271.183716	7758.433522	9.105856	-0.055391	4.744379
271.188944	7766.447422	9.110861	-0.055397	4.746755
271.446266	7774.524993	9.115866	-0.055450	4.749149
271.558718	7782.555596	9.120871	-0.055476	4.751528
271.765930	7790.571312	9.125875	-0.055520	4.753901
272.006172	7798.588336	9.130880	-0.055570	4.756273
272.097276	7806.633049	9.135885	-0.055592	4.758653
272.325383	7814.562010	9.140890	-0.055640	4.760996
272.808482	7822.564629	9.145895	-0.055735	4.763360
273.100330	7830.553205	9.150899	-0.055794	4.765718
273.447573	7838.576166	9.155904	-0.055864	4.768086
273.647954	7846.589750	9.160909	-0.055907	4.770450
273.801570	7854.625849	9.165914	-0.055940	4.772819
273.941093	7862.639342	9.170919	-0.055972	4.775181
274.142547	7870.675702	9.175923	-0.056014	4.777548
274.256602	7878.644972	9.180928	-0.056041	4.779895
274.439597	7886.715692	9.185933	-0.056080	4.782270
274.523235	7894.647956	9.190938	-0.056101	4.784603
274.670956	7902.766625	9.195943	-0.056134	4.786990
274.755138	7910.685571	9.200947	-0.056154	4.789317
274.973278	7918.775109	9.205952	-0.056200	4.791693
275.078762	7926.805419	9.210957	-0.056225	4.794050
275.237943	7934.816053	9.215962	-0.056260	4.796400
275.615237	7942.815866	9.220967	-0.056335	4.798745
275.727288	7950.818899	9.225971	-0.056361	4.801091
275.876297	7958.839255	9.230976	-0.056394	4.803441
275.895070	7966.823186	9.235981	-0.056403	4.805779
276.023453	7974.868222	9.240986	-0.056432	4.808134
276.046812	7982.836604	9.245991	-0.056442	4.810465
276.173993	7990.364243	9.250995	-0.056470	4.812666
276.611116	7995.162867	9.256000	-0.056555	4.814067
276.821986	7997.731925	9.261005	-0.056596	4.814817
276.890646	7999.044853	9.266010	-0.056609	4.815200
276.789540	7999.474785	9.271015	-0.056591	4.815326
276.899206	8000.629338	9.276019	-0.056612	4.815663
277.121052	8000.458836	9.281024	-0.056653	4.815612
277.298998	8000.533342	9.286029	-0.056686	4.815633
277.230824	8000.633716	9.291034	-0.056673	4.815663
277.450924	8000.565751	9.296039	-0.056714	4.815642
277.518135	8000.533734	9.301043	-0.056727	4.815632
277.494451	8000.535479	9.306048	-0.056722	4.815633
277.551019	8000.640042	9.311053	-0.056733	4.815663
277.572464	8000.510047	9.316058	-0.056737	4.815625
277.565411	8000.505655	9.321063	-0.056736	4.815624
277.545657	8000.649563	9.326067	-0.056732	4.815666
277.779207	8000.556177	9.331072	-0.056775	4.815638
277.665843	8000.528668	9.336077	-0.056754	4.815630
277.818255	8000.667930	9.341082	-0.056783	4.815670
277.863056	8000.451777	9.346087	-0.056791	4.815607
277.982433	8000.627890	9.351091	-0.056813	4.815658
278.009727	8000.413585	9.356096	-0.056818	4.815595
278.020623	8000.557998	9.361101	-0.056820	4.815637
278.188124	8000.547930	9.366106	-0.056851	4.815633
278.017569	8000.587859	9.371111	-0.056820	4.815646
277.923363	8000.595923	9.376115	-0.056802	4.815649
278.271471	8000.429632	9.381120	-0.056867	4.815598
278.199746	8000.459434	9.386125	-0.056853	4.815607
278.141516	8000.443516	9.391130	-0.056842	4.815603
278.189027	8000.418653	9.396135	-0.056851	4.815596
278.193351	8000.561890	9.401139	-0.056852	4.815637
278.245222	8000.459104	9.406144	-0.056862	4.815607
278.007929	8000.517167	9.411149	-0.056817	4.815625
278.184823	8000.495501	9.416154	-0.056850	4.815618
278.516659	8000.374884	9.421159	-0.056912	4.815581
278.362201	8000.449267	9.426163	-0.056883	4.815604
278.360664	8000.410777	9.431168	-0.056883	4.815592
278.335547	8000.522545	9.436173	-0.056878	4.815625
278.408850	8000.441480	9.441178	-0.056892	4.815601
278.551472	8000.541051	9.446183	-0.056919	4.815630
278.418722	8000.528180	9.451187	-0.056894	4.815626
278.669618	8000.441490	9.456192	-0.056940	4.815600
278.588189	8000.541648	9.461197	-0.056925	4.815630
278.823924	8000.445092	9.466202	-0.056969	4.815600
278.705527	8000.418568	9.471207	-0.056947	4.815593
278.475457	8000.568634	9.476211	-0.056904	4.815638
278.618699	8000.460941	9.481216	-0.056931	4.815606
278.735602	8000.475683	9.486221	-0.056953	4.815610
278.779962	8000.460384	9.491226	-0.056961	4.815605
278.755511	8000.441816	9.496231	-0.056956	4.815600
278.550493	8000.575200	9.501235	-0.056918	4.815640
278.690138	8000.334963	9.506240	-0.056944	4.815569
278.680012	8000.444841	9.511245	-0.056942	4.815601
278.671433	8000.405166	9.516250	-0.056940	4.815589
278.678193	8000.540965	9.521255	-0.056942	4.815629
278.728515	8000.431743	9.526259	-0.056951	4.815597
278.840193	8000.404731	9.531264	-0.056972	4.815588
278.895249	8000.432345	9.536269	-0.056982	4.815596
278.786339	8000.367514	9.541274	-0.056962	4.815578
278.985874	8000.254336	9.546279	-0.056999	4.815544
279.074594	8000.409647	9.551283	-0.057015	4.815589
279.100257	8000.406861	9.556288	-0.057020	4.815588
278.809526	8000.462976	9.561293	-0.056966	4.815606
278.979148	8000.520255	9.566298	-0.056998	4.815621
279.144145	8000.581732	9.571303	-0.057028	4.815639
278.973190	8000.444294	9.576307	-0.056996	4.815599
279.092675	8000.394973	9.581312	-0.057019	4.815584
279.095910	8000.534989	9.586317	-0.057019	4.815625
278.808918	8000.533469	9.591322	-0.056966	4.815626
278.853768	8000.602585	9.596327	-0.056974	4.815646
279.102598	8000.537229	9.601331	-0.057020	4.815626
279.089981	8000.558388	9.606336	-0.057018	4.815632
279.041308	8000.558653	9.611341	-0.057009	4.815632
279.024753	8000.544489	9.616346	-0.057006	4.815628
279.196168	8000.336825	9.621351	-0.057038	4.815567
279.010494	8000.527154	9.626355	-0.057003	4.815623
279.129044	8000.453244	9.631360	-0.057025	4.815601
279.089005	8000.554085	9.636365	-0.057018	4.815631
278.984388	8000.460475	9.641370	-0.056998	4.815604
279.101960	8000.403644	9.646375	-0.057020	4.815587
279.232026	8000.542542	9.651379	-0.057044	4.815627
279.399960	8000.445938	9.656384	-0.057075	4.815598
279.267244	8000.258913	9.661389	-0.057051	4.815544
279.139742	8000.378614	9.666394	-0.057027	4.815579
279.168496	8000.301090	9.671399	-0.057032	4.815557
279.266433	8000.367873	9.676403	-0.057050	4.815576
279.239336	8000.424052	9.681408	-0.057045	4.815592
279.367836	8000.351373	9.686413	-0.057069	4.815570
279.458183	8000.371021	9.691418	-0.057086	4.815576
279.420798	8000.305229	9.696423	-0.057079	4.815557
279.294034	8000.513623	9.701427	-0.057055	4.815618
279.596208	8000.342301	9.706432	-0.057112	4.815567
279.371036	8000.395221	9.711437	-0.057070	4.815583
279.393107	8000.445798	9.716442	-0.057074	4.815598
279.462923	8000.403139	9.721447	-0.057087	4.815585
279.443685	8000.526760	9.726451	-0.057083	4.815621
279.322159	8000.421118	9.731456	-0.057061	4.815591
279.453388	8000.295063	9.736461	-0.057085	4.815553
279.494736	8000.384422	9.741466	-0.057093	4.815579
279.597949	8000.365817	9.746471	-0.057112	4.815573
279.596652	8000.423490	9.751475	-0.057112	4.815590
279.677628	8000.403451	9.756480	-0.057127	4.815584
279.608792	8000.461081	9.761485	-0.057114	4.815601
279.542856	8000.438624	9.766490	-0.057101	4.815595
279.647981	8000.442489	9.771495	-0.057121	4.815596
279.533806	8000.400007	9.776499	-0.057100	4.815584
279.437489	8000.419789	9.781504	-0.057082	4.815590
279.666530	8000.559249	9.786509	-0.057124	4.815630
279.691253	8000.405797	9.791514	-0.057129	4.815585
279.795271	8000.441697	9.796519	-0.057148	4.815595
279.626734	8000.541492	9.801523	-0.057117	4.815625
279.897823	8000.314098	9.806528	-0.057167	4.815557
279.885954	8000.368391	9.811533	-0.057165	4.815573
279.820471	8000.418597	9.816538	-0.057153	4.815588
279.608577	8000.420449	9.821543	-0.057113	4.815589
279.770816	8000.476540	9.826547	-0.057144	4.815605
279.827911	8000.378111	9.831552	-0.057154	4.815576
279.647178	8000.609125	9.836557	-0.057121	4.815644
279.900821	8000.598340	9.841562	-0.057168	4.815640
279.987574	8000.417060	9.846567	-0.057184	4.815587
280.062335	8000.541161	9.851571	-0.057198	4.815622
280.019224	8000.569298	9.856576	-0.057190	4.815631
280.146998	8000.449594	9.861581	-0.057213	4.815595
280.072193	8000.550933	9.866586	-0.057200	4.815625
280.126279	8000.271885	9.871591	-0.057209	4.815543
280.183135	8000.421334	9.876595	-0.057220	4.815587
280.116084	8000.380695	9.881600	-0.057208	4.815575
280.224155	8000.426278	9.886605	-0.057228	4.815588
280.070796	8000.276305	9.891610	-0.057199	4.815545
280.097507	8000.266058	9.896615	-0.057204	4.815542
279.903881	8000.475491	9.901619	-0.057168	4.815604
279.874890	8000.444026	9.906624	-0.057163	4.815595
280.115528	8000.316565	9.911629	-0.057207	4.815557
280.026752	8000.419810	9.916634	-0.057191	4.815587
280.043243	8000.402984	9.921639	-0.057194	4.815582
280.116771	8000.340085	9.926643	-0.057207	4.815563
280.313470	8000.393538	9.931648	-0.057244	4.815578
280.110233	8000.526953	9.936653	-0.057206	4.815618
280.296879	8000.421040	9.941658	-0.057241	4.815586
280.350640	8000.399485	9.946663	-0.057251	4.815580
280.099504	8000.453046	9.951667	-0.057204	4.815596
280.058650	8000.367963	9.956672	-0.057196	4.815572
280.164172	8000.408162	9.961677	-0.057216	4.815583
280.119886	8000.435211	9.966682	-0.057208	4.815591
280.159516	8000.424108	9.971687	-0.057215	4.815588
280.260469	8000.482396	9.976691	-0.057234	4.815604
280.362802	8000.333425	9.981696	-0.057253	4.815560
280.329452	8000.559388	9.986701	-0.057247	4.815626
280.192608	8000.391521	9.991706	-0.057221	4.815578
280.384566	8000.557086	9.996711	-0.057257	4.815626
280.062293	8000.448137	10.001715	-0.057197	4.815595
280.159687	8000.437985	10.006720	-0.057215	4.815592
280.275198	8000.296711	10.011725	-0.057236	4.815550
280.365088	8000.356953	10.016730	-0.057253	4.815567
280.409085	8000.273267	10.021735	-0.057261	4.815542
280.115323	8000.416945	10.026739	-0.057207	4.815586
280.222200	8000.451824	10.031744	-0.057227	4.815596
280.226599	8000.416635	10.036749	-0.057227	4.815585
280.152977	8000.569280	10.041754	-0.057214	4.815630
280.402753	8000.271015	10.046759	-0.057260	4.815542
280.290861	8000.556587	10.051763	-0.057239	4.815626
280.255556	8000.278204	10.056768	-0.057233	4.815545
280.432828	8000.380486	10.061773	-0.057266	4.815574
280.228390	8000.430541	10.066778	-0.057228	4.815589
280.145238	8000.191974	10.071783	-0.057212	4.815520
280.271030	8000.369268	10.076787	-0.057235	4.815571
280.392401	8000.200311	10.081792	-0.057258	4.815521
280.204104	8000.346793	10.086797	-0.057223	4.815565
280.378609	8000.258844	10.091802	-0.057255	4.815538
280.474484	8000.360855	10.096807	-0.057273	4.815568
280.181189	8000.266275	10.101811	-0.057218	4.815542
280.223825	8000.369546	10.106816	-0.057226	4.815572
280.507920	8000.438328	10.111821	-0.057279	4.815590
280.474573	8000.543556	10.116826	-0.057273	4.815621
280.375381	8000.344254	10.121831	-0.057255	4.815563
280.544285	8000.404729	10.126835	-0.057286	4.815580
280.701588	8000.426549	10.131840	-0.057315	4.815586
280.509120	8000.252424	10.136845	-0.057279	4.815536
280.368700	8000.440297	10.141850	-0.057253	4.815592
280.538184	8000.395004	10.146855	-0.057285	4.815577
280.480964	8000.561809	10.151859	-0.057274	4.815626
280.239910	8000.534332	10.156864	-0.057229	4.815620
280.379129	8000.453281	10.161869	-0.057255	4.815595
280.457358	8000.559277	10.166874	-0.057270	4.815626
280.352482	8000.546863	10.171879	-0.057250	4.815623
280.479209	8000.374787	10.176883	-0.057274	4.815572
280.519774	8000.373316	10.181888	-0.057281	4.815571
280.431051	8000.431687	10.186893	-0.057265	4.815589
280.581329	8000.544211	10.191898	-0.057293	4.815621
280.660990	8000.263445	10.196903	-0.057307	4.815538
280.427942	8000.433766	10.201907	-0.057264	4.815589
280.502686	8000.277930	10.206912	-0.057278	4.815543
280.789083	8000.445050	10.211917	-0.057331	4.815591
280.765795	8000.430774	10.216922	-0.057327	4.815587
280.724720	8000.401247	10.221927	-0.057319	4.815578
280.539102	8000.440927	10.226931	-0.057285	4.815591
280.716187	8000.379732	10.231936	-0.057318	4.815572
280.494036	8000.408127	10.236941	-0.057276	4.815582
280.346276	8000.477279	10.241946	-0.057249	4.815602
280.380330	8000.465016	10.246951	-0.057255	4.815599
280.335721	8000.382007	10.251955	-0.057247	4.815575
280.590760	8000.428942	10.256960	-0.057294	4.815587
280.559988	8000.427365	10.261965	-0.057288	4.815587
280.449058	8000.558027	10.266970	-0.057268	4.815626
280.606966	8000.421723	10.271975	-0.057297	4.815585
280.748366	8000.361009	10.276979	-0.057323	4.815567
280.693658	8000.439173	10.281984	-0.057313	4.815590
280.553667	8000.287281	10.286989	-0.057287	4.815546
280.501391	8000.568494	10.291994	-0.057277	4.815628
280.858021	8000.310451	10.296999	-0.057344	4.815551
280.820497	8000.388897	10.302003	-0.057337	4.815574
280.688954	8000.473276	10.307008	-0.057312	4.815600
280.764234	8000.501225	10.312013	-0.057326	4.815607
280.623274	8000.543778	10.317018	-0.057300	4.815621
280.594159	8000.465297	10.322023	-0.057294	4.815598
280.540656	8000.528522	10.327027	-0.057284	4.815616
280.837149	8000.438308	10.332032	-0.057340	4.815589
280.853531	8000.459945	10.337037	-0.057343	4.815595
280.676940	8000.540376	10.342042	-0.057310	4.815619
280.890617	8000.263952	10.347047	-0.057349	4.815537
280.822620	8000.463703	10.352051	-0.057337	4.815596
280.632762	8000.532163	10.357056	-0.057301	4.815617
280.637141	8000.292895	10.362061	-0.057302	4.815547
280.562168	8000.360040	10.367066	-0.057288	4.815567
280.730102	8000.338228	10.372071	-0.057319	4.815560
280.742259	8000.474122	10.377075	-0.057322	4.815600
280.866198	8000.394956	10.382080	-0.057345	4.815576
280.804060	8000.365082	10.387085	-0.057333	4.815567
280.538168	8000.547685	10.392090	-0.057284	4.815622
280.763383	8000.245808	10.397095	-0.057325	4.815533
280.742723	8000.423900	10.402099	-0.057322	4.815585
280.697037	8000.439173	10.407104	-0.057313	4.815590
280.678237	8000.430313	10.412109	-0.057310	4.815587
280.778633	8000.505689	10.417114	-0.057328	4.815609
280.900984	8000.400854	10.422119	-0.057351	4.815577
280.745497	8000.529714	10.427123	-0.057322	4.815616
280.874233	8000.382245	10.432128	-0.057346	4.815572
281.074700	8000.541542	10.437133	-0.057383	4.815618
280.876373	8000.529725	10.442138	-0.057346	4.815615
280.713281	8000.555886	10.447143	-0.057316	4.815624
280.798081	8000.483555	10.452147	-0.057332	4.815602
280.848283	8000.505749	10.457152	-0.057341	4.815608
280.961597	8000.363368	10.462157	-0.057362	4.815566
280.698792	8000.547091	10.467162	-0.057313	4.815621
280.834059	8000.390113	10.472167	-0.057338	4.815575
280.696789	8000.351523	10.477171	-0.057313	4.815564
280.794423	8000.534769	10.482176	-0.057331	4.815617
280.827155	8000.353664	10.487181	-0.057337	4.815564
280.651114	8000.613609	10.492186	-0.057304	4.815641
280.738201	8000.329758	10.497191	-0.057320	4.815557
280.907296	8000.425497	10.502195	-0.057352	4.815585
280.649016	8000.566554	10.507200	-0.057304	4.815627
280.867258	8000.362861	10.512205	-0.057344	4.815567
280.690409	8000.502054	10.517210	-0.057311	4.815608
280.920396	8000.401128	10.522215	-0.057354	4.815577
280.962507	8000.422121	10.527219	-0.057362	4.815583
280.925598	8000.445017	10.532224	-0.057355	4.815590
281.021019	8000.436970	10.537229	-0.057373	4.815587
280.888169	8000.251003	10.542234	-0.057348	4.815534
280.921601	8000.333823	10.547239	-0.057354	4.815558
281.004359	8000.448442	10.552243	-0.057370	4.815591
281.036044	8000.544057	10.557248	-0.057376	4.815619
280.910779	8000.361418	10.562253	-0.057352	4.815566
280.893420	8000.554525	10.567258	-0.057349	4.815622
281.071541	8000.429238	10.572263	-0.057382	4.815585
280.882738	8000.547934	10.577267	-0.057347	4.815621
281.066956	8000.552034	10.582272	-0.057381	4.815621
281.198027	8000.306302	10.587277	-0.057405	4.815548
280.856707	8000.422486	10.592282	-0.057342	4.815584
280.953404	8000.289448	10.597287	-0.057360	4.815545
280.803309	8000.397028	10.602291	-0.057332	4.815577
281.099777	8000.433961	10.607296	-0.057387	4.815586
281.016936	8000.398404	10.612301	-0.057372	4.815576
280.898083	8000.562059	10.617306	-0.057350	4.815625
281.082686	8000.471070	10.622311	-0.057384	4.815597
281.119928	8000.498393	10.627315	-0.057391	4.815605
281.153001	8000.429484	10.632320	-0.057397	4.815585
281.302119	8000.424458	10.637325	-0.057425	4.815582
280.994723	8000.466407	10.642330	-0.057367	4.815596
281.086492	8000.304439	10.647335	-0.057384	4.815548
281.075090	8000.404686	10.652339	-0.057382	4.815578
281.298745	8000.458585	10.657344	-0.057424	4.815592
281.330748	8000.201606	10.662349	-0.057430	4.815517
281.035478	8000.364493	10.667354	-0.057375	4.815566
281.205062	8000.223039	10.672359	-0.057406	4.815524
281.160821	8000.424250	10.677363	-0.057398	4.815583
281.109117	8000.295179	10.682368	-0.057388	4.815546
281.214632	8000.247765	10.687373	-0.057408	4.815531
281.115464	8000.468373	10.692378	-0.057390	4.815596
281.150053	8000.340723	10.697383	-0.057396	4.815559
281.086044	8000.224271	10.702387	-0.057384	4.815525
281.275284	8000.155797	10.707392	-0.057419	4.815504
281.124265	8000.430044	10.712397	-0.057391	4.815585
281.011436	8000.309583	10.717402	-0.057370	4.815550
281.385558	8000.308261	10.722407	-0.057440	4.815548
281.169874	8000.218161	10.727411	-0.057399	4.815523
281.148057	8000.322510	10.732416	-0.057395	4.815553
281.201744	8000.269968	10.737421	-0.057405	4.815538
281.016556	8000.433599	10.742426	-0.057371	4.815587
281.095818	8000.304548	10.747431	-0.057386	4.815548
281.188904	8000.357365	10.752435	-0.057403	4.815563
281.097206	8000.300292	10.757440	-0.057386	4.815547
281.020563	8000.410149	10.762445	-0.057372	4.815580
281.174594	8000.460765	10.767450	-0.057400	4.815594
281.389223	8000.458955	10.772455	-0.057440	4.815592
281.268498	8000.334089	10.777459	-0.057418	4.815556
281.085735	8000.403734	10.782464	-0.057384	4.815577
281.470366	8000.408998	10.787469	-0.057455	4.815577
281.257571	8000.369162	10.792474	-0.057415	4.815567
281.159274	8000.340830	10.797479	-0.057397	4.815559
281.177749	8000.438363	10.802483	-0.057401	4.815587
281.373661	8000.402054	10.807488	-0.057437	4.815576
281.063563	8000.445026	10.812493	-0.057379	4.815590
281.042810	8000.462847	10.817498	-0.057375	4.815595
281.270633	8000.358679	10.822503	-0.057418	4.815563
281.281907	8000.514862	10.827507	-0.057420	4.815609
281.138290	8000.470823	10.832512	-0.057393	4.815597
281.360946	8000.421063	10.837517	-0.057435	4.815581
281.291885	8000.393212	10.842522	-0.057422	4.815573
281.277310	8000.255136	10.847527	-0.057419	4.815533
281.336528	8000.433476	10.852531	-0.057430	4.815585
281.305280	8000.440439	10.857536	-0.057424	4.815587
281.210594	8000.211292	10.862541	-0.057406	4.815521
281.213523	8000.409006	10.867546	-0.057407	4.815578
281.343169	8000.286126	10.872551	-0.057431	4.815542
281.255717	8000.257972	10.877555	-0.057415	4.815534
281.169004	8000.258679	10.882560	-0.057398	4.815535
281.311598	8000.223628	10.887565	-0.057425	4.815524
281.312240	8000.341169	10.892570	-0.057425	4.815558
281.271752	8000.248611	10.897575	-0.057418	4.815531
281.085379	8000.391921	10.902579	-0.057383	4.815574
281.250562	8000.370064	10.907584	-0.057414	4.815567
281.276689	8000.264712	10.912589	-0.057418	4.815536
281.332685	8000.405603	10.917594	-0.057429	4.815577
281.443716	8000.256773	10.922599	-0.057449	4.815533
281.413729	8000.217812	10.927603	-0.057444	4.815522
281.146202	8000.411073	10.932608	-0.057394	4.815579
281.344902	8000.192100	10.937613	-0.057431	4.815514
281.259917	8000.290066	10.942618	-0.057415	4.815543
281.537639	8000.218775	10.947623	-0.057467	4.815521
281.416996	8000.190074	10.952627	-0.057444	4.815513
281.215514	8000.188892	10.957632	-0.057407	4.815514
281.277310	8000.192044	10.962637	-0.057418	4.815515
281.378028	8000.287726	10.967642	-0.057437	4.815542
281.348685	8000.162229	10.972647	-0.057431	4.815506
281.380909	8000.238619	10.977651	-0.057437	4.815528
281.155809	8000.480661	10.982656	-0.057396	4.815600
281.587458	8000.203550	10.987661	-0.057476	4.815517
281.256299	8000.560311	10.992666	-0.057414	4.815622
281.305805	8000.399782	10.997671	-0.057423	4.815575
281.289557	8000.290527	11.002675	-0.057420	4.815543
281.384713	8000.440611	11.007680	-0.057438	4.815587
281.503356	8000.339988	11.012685	-0.057460	4.815557
281.436421	8000.378418	11.017690	-0.057448	4.815568
281.502101	8000.170075	11.022695	-0.057460	4.815507
281.322970	8000.519722	11.027699	-0.057427	4.815610
281.339160	8000.206921	11.032704	-0.057429	4.815519
281.310865	8000.350697	11.037709	-0.057424	4.815561
281.309153	8000.347462	11.042714	-0.057424	4.815560
281.217930	8000.326725	11.047719	-0.057407	4.815554
281.183864	8000.427667	11.052723	-0.057400	4.815584
281.349003	8000.411152	11.057728	-0.057431	4.815578
281.284972	8000.323548	11.062733	-0.057419	4.815553
281.114825	8000.321813	11.067738	-0.057387	4.815553
281.416124	8000.385538	11.072743	-0.057444	4.815571
281.421873	8000.286262	11.077747	-0.057445	4.815542
281.110144	8000.458494	11.082752	-0.057387	4.815593
281.209689	8000.275284	11.087757	-0.057405	4.815539
281.399794	8000.446164	11.092762	-0.057440	4.815588
281.443230	8000.447946	11.097767	-0.057449	4.815589
281.245120	8000.389119	11.102771	-0.057412	4.815572
281.093334	8000.553301	11.107776	-0.057383	4.815621
281.388992	8000.252582	11.112781	-0.057438	4.815532
281.252771	8000.528142	11.117786	-0.057413	4.815613
281.289518	8000.232775	11.122791	-0.057420	4.815527
281.537203	8000.434521	11.127795	-0.057466	4.815584
281.356436	8000.443295	11.132800	-0.057432	4.815588
281.445813	8000.268465	11.137805	-0.057449	4.815536
281.423353	8000.406996	11.142810	-0.057445	4.815577
281.625387	8000.148542	11.147815	-0.057482	4.815500
281.278390	8000.359727	11.152819	-0.057418	4.815564
281.205156	8000.304027	11.157824	-0.057404	4.815548
281.587403	8000.189580	11.162829	-0.057475	4.815513
281.501176	8000.358047	11.167834	-0.057459	4.815562
281.386219	8000.486507	11.172839	-0.057438	4.815600
281.385209	8000.267449	11.177843	-0.057437	4.815536
281.412748	8000.410008	11.182848	-0.057442	4.815578
281.556434	8000.212566	11.187853	-0.057469	4.815519
281.487670	8000.474279	11.192858	-0.057456	4.815596
281.529956	8000.287988	11.197863	-0.057464	4.815542
281.562008	8000.398567	11.202867	-0.057470	4.815574
281.633456	8000.383714	11.207872	-0.057483	4.815569
281.558235	8000.349350	11.212877	-0.057469	4.815559
281.575796	8000.580432	11.217882	-0.057473	4.815627
281.435278	8000.392197	11.222887	-0.057446	4.815572
281.515599	8000.417025	11.227891	-0.057461	4.815579
281.430184	8000.443396	11.232896	-0.057445	4.815587
281.504161	8000.319599	11.237901	-0.057459	4.815551
281.442518	8000.380554	11.242906	-0.057448	4.815569
281.612626	8000.261546	11.247911	-0.057479	4.815533
281.527735	8000.392638	11.252915	-0.057463	4.815572
281.412097	8000.393937	11.257920	-0.057442	4.815573
281.641725	8000.507771	11.262925	-0.057485	4.815605
281.703666	8000.342104	11.267930	-0.057496	4.815557
281.680847	8000.328904	11.272935	-0.057492	4.815553
281.552966	8000.272303	11.277939	-0.057468	4.815537
281.307567	8000.318479	11.282944	-0.057422	4.815552
281.621762	8000.148419	11.287949	-0.057481	4.815500
281.451485	8000.558049	11.292954	-0.057449	4.815621
281.512259	8000.321843	11.297959	-0.057460	4.815552
281.448748	8000.444739	11.302963	-0.057449	4.815588
281.444791	8000.521603	11.307968	-0.057448	4.815610
281.653150	8000.447033	11.312973	-0.057487	4.815587
281.753269	8000.451885	11.317978	-0.057505	4.815588
281.575416	8000.443611	11.322983	-0.057472	4.815587
281.693104	8000.233986	11.327987	-0.057494	4.815525
281.713824	8000.430927	11.332992	-0.057498	4.815582
281.751687	8000.049031	11.337997	-0.057505	4.815471
281.531988	8000.417243	11.343002	-0.057464	4.815579
281.757483	8000.087587	11.348007	-0.057506	4.815482
281.735862	8000.443035	11.353011	-0.057502	4.815586
281.731388	8000.457918	11.358016	-0.057501	4.815590
281.839896	8000.191511	11.363021	-0.057521	4.815512
281.686815	8000.328960	11.368026	-0.057492	4.815553
281.507270	8000.167866	11.373031	-0.057459	4.815507
281.635595	8000.108005	11.378035	-0.057483	4.815488
281.691864	8000.245694	11.383040	-0.057493	4.815528
281.687258	8000.357807	11.388045	-0.057492	4.815561
281.502370	8000.316295	11.393050	-0.057458	4.815550
281.625800	8000.270243	11.398055	-0.057481	4.815536
281.518297	8000.416990	11.403059	-0.057461	4.815579
281.550678	8000.523303	11.408064	-0.057467	4.815610
281.808980	8000.199528	11.413069	-0.057515	4.815514
281.729142	8000.436484	11.418074	-0.057500	4.815584
281.538789	8000.272005	11.423079	-0.057465	4.815537
281.591293	8000.310264	11.428083	-0.057474	4.815548
281.663845	8000.354196	11.433088	-0.057488	4.815560
281.722609	8000.242970	11.438093	-0.057499	4.815528
281.517991	8000.314393	11.443098	-0.057461	4.815549
281.617690	8000.139733	11.448103	-0.057479	4.815498
281.827349	8000.270332	11.453107	-0.057518	4.815535
281.776558	8000.396644	11.458112	-0.057509	4.815572
281.787290	8000.431011	11.463117	-0.057511	4.815582
281.742966	8000.408908	11.468122	-0.057502	4.815576
281.809185	8000.241175	11.473127	-0.057515	4.815527
281.565597	7999.994618	11.478131	-0.057469	4.815456
281.399791	8000.047447	11.483136	-0.057438	4.815472
281.607017	8000.004912	11.488141	-0.057477	4.815459
281.409139	8000.111704	11.493146	-0.057440	4.815491
281.407412	8000.202494	11.498151	-0.057440	4.815517
281.320649	8000.127339	11.503155	-0.057423	4.815496
281.406498	8000.189653	11.508160	-0.057439	4.815513
281.480764	8000.118217	11.513165	-0.057453	4.815492
281.616749	8000.152508	11.518170	-0.057479	4.815502
281.645560	8000.305773	11.523175	-0.057484	4.815546
281.584163	8000.041914	11.528179	-0.057472	4.815469
281.471462	8000.184300	11.533184	-0.057451	4.815512
281.469982	8000.069947	11.538189	-0.057451	4.815478
281.326784	8000.138106	11.543194	-0.057424	4.815499
281.451508	8000.103829	11.548199	-0.057448	4.815488
281.490401	8000.041428	11.553203	-0.057455	4.815470
281.543422	8000.418403	11.558208	-0.057465	4.815580
281.678621	8000.063754	11.563213	-0.057490	4.815475
281.490380	8000.209171	11.568218	-0.057455	4.815519
281.501029	8000.274521	11.573223	-0.057457	4.815538
281.425504	8000.169633	11.578227	-0.057443	4.815508
281.368666	8000.249899	11.583232	-0.057432	4.815531
281.424164	8000.353385	11.588237	-0.057442	4.815561
281.451743	8000.237372	11.593242	-0.057447	4.815527
281.353623	8000.285973	11.598247	-0.057429	4.815542
281.404472	8000.190645	11.603251	-0.057439	4.815514
281.297954	8000.505160	11.608256	-0.057419	4.815606
281.414512	8000.184395	11.613261	-0.057440	4.815512
281.581025	8000.344201	11.618266	-0.057472	4.815558
281.718918	8000.102856	11.623271	-0.057497	4.815487
281.561623	8000.141934	11.628275	-0.057468	4.815499
281.594356	8000.454469	11.633280	-0.057474	4.815590
281.804673	8000.165164	11.638285	-0.057513	4.815504
281.381720	8000.333429	11.643290	-0.057434	4.815556
281.602119	8000.366973	11.648295	-0.057475	4.815564
281.585571	8000.208563	11.653299	-0.057472	4.815518
281.525661	8000.388148	11.658304	-0.057461	4.815571
281.419112	8000.314803	11.663309	-0.057441	4.815550
281.430281	8000.328875	11.668314	-0.057443	4.815554
281.466153	8000.208725	11.673319	-0.057450	4.815519
281.438159	8000.551246	11.678323	-0.057445	4.815619
281.488458	8000.463387	11.683328	-0.057454	4.815593
281.642721	8000.275734	11.688333	-0.057483	4.815537
281.577017	8000.411416	11.693338	-0.057470	4.815577
281.453871	8000.199964	11.698343	-0.057447	4.815516
281.571713	8000.223271	11.703347	-0.057469	4.815523
281.380403	8000.264995	11.708352	-0.057434	4.815536
281.546069	8000.247419	11.713357	-0.057464	4.815530
281.447997	8000.259693	11.718362	-0.057446	4.815534
281.544905	8000.223889	11.723367	-0.057464	4.815523
281.587750	8000.379523	11.728371	-0.057472	4.815568
281.503682	8000.283041	11.733376	-0.057456	4.815540
281.603729	8000.270796	11.738381	-0.057475	4.815536
281.375370	8000.560867	11.743386	-0.057433	4.815622
281.466745	8000.413850	11.748391	-0.057450	4.815579
281.763774	8000.350356	11.753395	-0.057505	4.815559
281.739319	8000.407650	11.758400	-0.057500	4.815576
281.727261	8000.148875	11.763405	-0.057498	4.815500
281.430846	8000.204895	11.768410	-0.057443	4.815518
281.507200	8000.128152	11.773415	-0.057457	4.815495
281.508118	8000.181588	11.778419	-0.057457	4.815511
281.463129	8000.200078	11.783424	-0.057449	4.815516
281.562439	8000.196368	11.788429	-0.057467	4.815515
281.567916	8000.339633	11.793434	-0.057468	4.815557
281.558502	8000.448462	11.798439	-0.057466	4.815588
281.564364	8000.421844	11.803443	-0.057468	4.815581
281.723323	8000.202214	11.808448	-0.057497	4.815516
281.648009	8000.157164	11.813453	-0.057483	4.815503
281.524272	8000.421177	11.818458	-0.057460	4.815581
281.490352	8000.420616	11.823463	-0.057454	4.815581
281.495799	8000.430320	11.828467	-0.057455	4.815583
281.403464	8000.308058	11.833472	-0.057437	4.815548
281.527994	8000.269504	11.838477	-0.057460	4.815536
281.484760	8000.475008	11.843482	-0.057453	4.815596
281.366872	8000.355530	11.848487	-0.057430	4.815562
281.586410	8000.171090	11.853491	-0.057471	4.815507
281.569694	8000.367414	11.858496	-0.057468	4.815565
281.629038	8000.120501	11.863501	-0.057479	4.815492
281.441823	8000.294783	11.868506	-0.057444	4.815544
281.811192	8000.109605	11.873511	-0.057513	4.815488
281.810370	8000.248492	11.878515	-0.057513	4.815529
281.663427	8000.361467	11.883520	-0.057486	4.815562
281.734151	8000.156412	11.888525	-0.057499	4.815502
281.754082	8000.429202	11.893530	-0.057502	4.815582
281.548311	8000.223867	11.898535	-0.057464	4.815523
281.810890	8000.227120	11.903539	-0.057513	4.815523
281.581988	8000.425292	11.908544	-0.057470	4.815582
281.536852	8000.201233	11.913549	-0.057462	4.815516
281.732163	8000.449131	11.918554	-0.057498	4.815588
281.827827	8000.371636	11.923559	-0.057516	4.815565
281.763508	8000.306465	11.928563	-0.057504	4.815546
281.605389	8000.184189	11.933568	-0.057474	4.815511
281.828217	8000.137637	11.938573	-0.057516	4.815496
281.850393	8000.367725	11.943578	-0.057520	4.815563
281.662596	8000.199014	11.948583	-0.057485	4.815515
281.627386	8000.223007	11.953587	-0.057478	4.815522
281.765273	8000.402645	11.958592	-0.057504	4.815574
281.906729	8000.213712	11.963597	-0.057530	4.815518
281.727630	8000.232130	11.968602	-0.057497	4.815524
281.679145	8000.306124	11.973607	-0.057488	4.815546
281.562343	8000.392883	11.978611	-0.057466	4.815572
281.615535	8000.399099	11.983616	-0.057476	4.815574
281.694145	8000.134338	11.988621	-0.057491	4.815496
281.644984	8000.409196	11.993626	-0.057482	4.815577
281.589283	8000.239455	11.998631	-0.057471	4.815527
281.593805	8000.221363	12.003635	-0.057472	4.815522
281.564964	8000.446337	12.008640	-0.057467	4.815588
281.534480	8000.242820	12.013645	-0.057461	4.815528
281.523644	8000.331323	12.018650	-0.057459	4.815554
281.761887	8000.423930	12.023655	-0.057503	4.815580
281.749913	8000.478224	12.028659	-0.057501	4.815596
281.675598	8000.476997	12.033664	-0.057487	4.815596
281.860057	8000.075076	12.038669	-0.057521	4.815478
281.726149	8000.356017	12.043674	-0.057496	4.815561
281.758043	8000.406759	12.048679	-0.057502	4.815575
281.729996	8000.427665	12.053683	-0.057497	4.815582
281.822352	8000.382170	12.058688	-0.057514	4.815568
281.735769	8000.285646	12.063693	-0.057498	4.815540
281.700536	8000.316050	12.068698	-0.057491	4.815549
281.566073	8000.313833	12.073703	-0.057466	4.815549
281.716683	8000.286394	12.078707	-0.057494	4.815540
281.595323	8000.388036	12.083712	-0.057472	4.815571
281.539547	8000.232185	12.088717	-0.057461	4.815525
281.639992	8000.420822	12.093722	-0.057480	4.815580
281.581683	8000.389942	12.098727	-0.057469	4.815571
281.746099	8000.280456	12.103731	-0.057500	4.815538
281.671185	8000.427740	12.108736	-0.057486	4.815582
281.715501	8000.402824	12.113741	-0.057494	4.815574
281.692973	8000.321245	12.118746	-0.057490	4.815551
281.843029	8000.302345	12.123751	-0.057518	4.815544
281.664626	8000.151954	12.128755	-0.057484	4.815501
281.593718	8000.442480	12.133760	-0.057471	4.815587
281.819270	8000.283782	12.138765	-0.057513	4.815539
281.616377	8000.236631	12.143770	-0.057475	4.815526
281.751618	8000.438664	12.148775	-0.057501	4.815585
281.721721	8000.426415	12.153779	-0.057495	4.815581
281.834463	8000.440024	12.158784	-0.057516	4.815585
281.740963	8000.156400	12.163789	-0.057498	4.815502
281.614674	8000.318865	12.168794	-0.057475	4.815550
281.591828	8000.335582	12.173799	-0.057471	4.815555
281.735096	8000.325118	12.178803	-0.057497	4.815552
281.745218	8000.354131	12.183808	-0.057499	4.815560
281.706459	8000.201766	12.188813	-0.057492	4.815516
281.784179	8000.258604	12.193818	-0.057506	4.815532
281.657178	8000.422127	12.198823	-0.057483	4.815580
281.891533	8000.390724	12.203827	-0.057526	4.815570
281.752246	8000.292263	12.208832	-0.057500	4.815542
281.846541	8000.329074	12.213837	-0.057518	4.815552
281.675286	8000.307019	12.218842	-0.057486	4.815547
281.786138	8000.314185	12.223847	-0.057507	4.815548
281.915013	8000.314168	12.228851	-0.057531	4.815547
281.711536	8000.381335	12.233856	-0.057493	4.815568
281.825063	8000.327641	12.238861	-0.057514	4.815552
281.850430	8000.222276	12.243866	-0.057518	4.815521
281.848228	8000.396402	12.248871	-0.057518	4.815572
281.697272	8000.226160	12.253875	-0.057490	4.815523
281.773263	8000.238094	12.258880	-0.057504	4.815526
281.920813	8000.374083	12.263885	-0.057532	4.815565
281.744030	8000.269663	12.268890	-0.057499	4.815535
281.630349	8000.370363	12.273895	-0.057477	4.815565
281.933590	8000.156315	12.278899	-0.057534	4.815501
281.727946	8000.161475	12.283904	-0.057495	4.815504
281.974261	8000.096077	12.288909	-0.057541	4.815483
281.894853	8000.359752	12.293914	-0.057527	4.815561
281.763152	8000.302019	12.298919	-0.057502	4.815545
281.649373	8000.191158	12.303923	-0.057481	4.815513
281.776875	8000.418706	12.308928	-0.057505	4.815579
281.730713	8000.248054	12.313933	-0.057496	4.815529
281.698778	8000.354374	12.318938	-0.057490	4.815560
281.666534	8000.279047	12.323943	-0.057484	4.815538
281.671633	8000.163733	12.328947	-0.057485	4.815505
281.748586	8000.417161	12.333952	-0.057499	4.815578
281.723917	8000.281054	12.338957	-0.057494	4.815539
281.759457	8000.487856	12.343962	-0.057501	4.815599
281.794091	8000.437136	12.348967	-0.057508	4.815584
281.794309	8000.301439	12.353971	-0.057507	4.815544
281.791755	8000.426408	12.358976	-0.057507	4.815581
281.785914	8000.345104	12.363981	-0.057506	4.815557
281.722670	8000.466937	12.368986	-0.057494	4.815593
281.541239	8000.403043	12.373991	-0.057460	4.815575
281.711677	8000.249848	12.378995	-0.057492	4.815530
281.699231	8000.251778	12.384000	-0.057490	4.815530
281.788021	8000.386799	12.389005	-0.057506	4.815569
281.902140	8000.448513	12.394010	-0.057527	4.815587
281.805561	8000.273823	12.399015	-0.057509	4.815536
281.689039	8000.190698	12.404019	-0.057488	4.815513
281.621199	8000.382974	12.409024	-0.057475	4.815569
281.820307	8000.294361	12.414029	-0.057512	4.815542
281.862452	8000.530122	12.419034	-0.057520	4.815611
281.923368	8000.358026	12.424039	-0.057531	4.815560
281.920189	8000.279972	12.429043	-0.057531	4.815537
281.789072	8000.377180	12.434048	-0.057506	4.815567
281.837492	8000.272194	12.439053	-0.057515	4.815536
281.794392	8000.259729	12.444058	-0.057507	4.815532
281.801456	8000.234199	12.449063	-0.057508	4.815525
281.895421	8000.080814	12.454067	-0.057526	4.815479
281.705242	8000.375788	12.459072	-0.057490	4.815567
281.964225	8000.268928	12.464077	-0.057539	4.815534
281.986228	8000.368658	12.469082	-0.057543	4.815563
281.796127	8000.409333	12.474087	-0.057507	4.815576
282.021050	8000.190789	12.479091	-0.057549	4.815511
281.799562	8000.411522	12.484096	-0.057508	4.815577
281.740287	8000.207530	12.489101	-0.057497	4.815517
281.803217	8000.358153	12.494106	-0.057508	4.815561
281.846863	8000.307582	12.499111	-0.057517	4.815546
281.927745	8000.254419	12.504115	-0.057532	4.815530
281.896101	8000.524225	12.509120	-0.057526	4.815609
282.082429	8000.254825	12.514125	-0.057560	4.815529
281.956468	8000.255953	12.519130	-0.057537	4.815530
281.892815	8000.165150	12.524135	-0.057525	4.815504
282.118686	8000.192374	12.529139	-0.057567	4.815511
282.044296	8000.354626	12.534144	-0.057553	4.815559
281.971624	8000.243372	12.539149	-0.057539	4.815527
281.903735	8000.419622	12.544154	-0.057527	4.815578
281.916449	8000.396322	12.549159	-0.057529	4.815572
282.076749	8000.377590	12.554163	-0.057559	4.815565
281.696956	8000.377743	12.559168	-0.057488	4.815567
282.014130	8000.277184	12.564173	-0.057547	4.815536
282.067079	8000.225698	12.569178	-0.057557	4.815521
281.929226	8000.331343	12.574183	-0.057531	4.815552
281.886137	8000.300713	12.579187	-0.057523	4.815544
281.867199	8000.570730	12.584192	-0.057520	4.815623
282.058612	8000.053523	12.589197	-0.057555	4.815471
281.905845	8000.213415	12.594202	-0.057527	4.815518
281.771416	8000.276377	12.599207	-0.057502	4.815537
281.942064	8000.384966	12.604211	-0.057534	4.815568
281.833300	8000.330816	12.609216	-0.057513	4.815553
282.050368	8000.335457	12.614221	-0.057554	4.815553
282.078823	8000.306006	12.619226	-0.057559	4.815544
282.108928	8000.284061	12.624231	-0.057565	4.815538
281.973687	8000.264736	12.629235	-0.057539	4.815533
281.870439	8000.258759	12.634240	-0.057520	4.815532
281.939136	8000.236381	12.639245	-0.057533	4.815525
281.915819	8000.335365	12.644250	-0.057529	4.815554
281.960273	8000.285876	12.649255	-0.057537	4.815539
282.090943	8000.072191	12.654259	-0.057561	4.815476
281.865141	8000.522579	12.659264	-0.057519	4.815609
282.053545	8000.325871	12.664269	-0.057554	4.815550
282.132628	8000.345336	12.669274	-0.057569	4.815556
281.836152	8000.336176	12.674279	-0.057514	4.815554
281.913846	8000.250906	12.679283	-0.057528	4.815529
282.045547	8000.394114	12.684288	-0.057553	4.815570
282.047127	8000.131289	12.689293	-0.057553	4.815493
281.993489	8000.315252	12.694298	-0.057543	4.815547
281.972196	8000.240104	12.699303	-0.057539	4.815526
282.067520	8000.185042	12.704307	-0.057556	4.815509
281.868044	8000.366604	12.709312	-0.057519	4.815563
282.004887	8000.223540	12.714317	-0.057545	4.815521
282.024120	8000.231334	12.719322	-0.057548	4.815523
281.828959	8000.302912	12.724327	-0.057512	4.815545
281.959294	8000.230262	12.729331	-0.057536	4.815523
281.902298	8000.243211	12.734336	-0.057526	4.815527
282.118775	8000.139925	12.739341	-0.057566	4.815496
281.946226	8000.405273	12.744346	-0.057534	4.815574
281.838536	8000.141717	12.749351	-0.057514	4.815498
281.811719	8000.117767	12.754355	-0.057509	4.815491
281.795663	8000.335471	12.759360	-0.057506	4.815554
282.053396	8000.241412	12.764365	-0.057554	4.815526
282.092359	8000.024081	12.769370	-0.057561	4.815462
281.842477	8000.333030	12.774375	-0.057514	4.815553
282.047517	8000.293665	12.779379	-0.057552	4.815541
282.045831	8000.342786	12.784384	-0.057552	4.815555
282.211550	8000.160663	12.789389	-0.057583	4.815501
282.158836	8000.335026	12.794394	-0.057573	4.815552
281.941587	8000.280158	12.799399	-0.057533	4.815537
282.188717	7999.974364	12.804403	-0.057578	4.815447
282.052126	8000.273426	12.809408	-0.057553	4.815535
282.141686	8000.165913	12.814413	-0.057570	4.815503
281.958370	8000.034674	12.819418	-0.057535	4.815466
281.944278	8000.364602	12.824423	-0.057533	4.815562
282.133117	8000.081354	12.829427	-0.057568	4.815478
282.037560	8000.265696	12.834432	-0.057550	4.815533
282.020047	8000.106200	12.839437	-0.057547	4.815486
282.117897	8000.130247	12.844442	-0.057565	4.815493
282.157898	8000.282630	12.849447	-0.057573	4.815537
282.307157	7999.997662	12.854451	-0.057600	4.815453
282.103932	8000.240065	12.859456	-0.057563	4.815525
282.092508	8000.167217	12.864461	-0.057560	4.815504
282.039184	8000.224035	12.869466	-0.057550	4.815521
282.099648	8000.308372	12.874471	-0.057562	4.815545
282.054747	7999.949687	12.879475	-0.057553	4.815440
281.974838	8000.251818	12.884480	-0.057538	4.815529
282.205082	7999.994897	12.889485	-0.057581	4.815453
282.047016	8000.104483	12.894490	-0.057552	4.815486
281.988861	8000.156947	12.899495	-0.057541	4.815501
282.158337	7999.911848	12.904499	-0.057572	4.815429
281.815621	8000.224610	12.909504	-0.057509	4.815522
281.821730	8000.247146	12.914509	-0.057510	4.815528
282.043547	8000.174934	12.919514	-0.057551	4.815506
281.975232	8000.256081	12.924519	-0.057538	4.815530
281.853889	8000.165396	12.929523	-0.057516	4.815504
281.807612	8000.214850	12.934528	-0.057507	4.815519
281.927472	8000.238192	12.939533	-0.057529	4.815525
281.993725	8000.217911	12.944538	-0.057542	4.815519
281.872260	8000.394346	12.949543	-0.057519	4.815571
282.250468	8000.176189	12.954547	-0.057589	4.815506
282.151438	8000.237597	12.959552	-0.057571	4.815524
282.098197	8000.353184	12.964557	-0.057561	4.815558
282.017553	8000.086868	12.969562	-0.057546	4.815481
282.036016	8000.344676	12.974567	-0.057549	4.815556
282.033188	8000.211065	12.979571	-0.057549	4.815517
281.972084	8000.290194	12.984576	-0.057537	4.815540
281.997384	8000.331211	12.989581	-0.057542	4.815552
282.109597	8000.151413	12.994586	-0.057563	4.815499
281.991077	8000.264856	12.999591	-0.057541	4.815533
282.051110	8000.068172	13.004595	-0.057552	4.815475
281.991855	8000.330042	13.009600	-0.057541	4.815552
282.057618	8000.202904	13.014605	-0.057553	4.815514
282.154982	8000.216259	13.019610	-0.057571	4.815518
282.101385	8000.366032	13.024615	-0.057561	4.815562
282.166365	8000.192935	13.029619	-0.057573	4.815511
281.893946	8000.361542	13.034624	-0.057523	4.815562
282.229884	8000.139483	13.039629	-0.057585	4.815495
281.981226	8000.368318	13.044634	-0.057539	4.815563
281.901065	8000.330666	13.049639	-0.057524	4.815552
281.913937	8000.232575	13.054643	-0.057526	4.815524
281.955969	8000.231128	13.059648	-0.057534	4.815523
281.918494	8000.153577	13.064653	-0.057527	4.815501
281.980394	8000.044541	13.069658	-0.057538	4.815468
282.143685	8000.338925	13.074663	-0.057569	4.815554
282.155901	8000.158548	13.079667	-0.057571	4.815501
281.834839	8000.355203	13.084672	-0.057511	4.815560
281.896171	8000.273937	13.089677	-0.057523	4.815536
282.027403	8000.244042	13.094682	-0.057547	4.815527
281.965970	8000.379795	13.099687	-0.057536	4.815567
282.213475	8000.206499	13.104691	-0.057582	4.815515
282.043343	8000.245366	13.109696	-0.057550	4.815527
282.024984	8000.304897	13.114701	-0.057547	4.815544
282.126053	8000.202916	13.119706	-0.057565	4.815514
282.126444	8000.279851	13.124711	-0.057565	4.815537
282.231734	8000.027282	13.129715	-0.057585	4.815462
282.181494	8000.303192	13.134720	-0.057576	4.815543
282.270864	8000.339922	13.139725	-0.057592	4.815553
282.287006	8000.063446	13.144730	-0.057595	4.815473
281.951808	8000.226745	13.149735	-0.057533	4.815522
282.274457	8000.245947	13.154739	-0.057593	4.815526
282.057553	8000.332126	13.159744	-0.057552	4.815552
282.007459	8000.222312	13.164749	-0.057543	4.815520
281.931299	8000.276617	13.169754	-0.057529	4.815537
282.073018	8000.267195	13.174759	-0.057555	4.815533
282.055504	8000.070303	13.179763	-0.057552	4.815476
282.076242	8000.149710	13.184768	-0.057556	4.815499
282.139521	8000.200969	13.189773	-0.057567	4.815513
282.170124	8000.119197	13.194778	-0.057573	4.815489
282.079832	8000.191434	13.199783	-0.057556	4.815511
282.013275	8000.069597	13.204787	-0.057544	4.815476
282.263018	8000.117514	13.209792	-0.057590	4.815488
282.084694	8000.206466	13.214797	-0.057557	4.815515
282.093015	8000.248272	13.219802	-0.057559	4.815528
282.112437	8000.374672	13.224807	-0.057562	4.815564
282.163731	8000.219514	13.229811	-0.057572	4.815519
281.895634	8000.246083	13.234816	-0.057522	4.815528
282.003484	8000.190158	13.239821	-0.057542	4.815511
282.167388	8000.159732	13.244826	-0.057572	4.815501
281.968114	8000.253681	13.249831	-0.057535	4.815530
281.988706	8000.142895	13.254835	-0.057539	4.815497
282.060169	8000.213521	13.259840	-0.057552	4.815518
282.198883	8000.201913	13.264845	-0.057578	4.815513
282.044068	8000.026267	13.269850	-0.057549	4.815463
282.105708	8000.313634	13.274855	-0.057561	4.815547
282.119226	8000.112978	13.279859	-0.057563	4.815488
282.044257	8000.418399	13.284864	-0.057549	4.815577
282.051492	8000.224050	13.289869	-0.057551	4.815521
282.177691	8000.157742	13.294874	-0.057574	4.815501
281.947955	8000.384751	13.299879	-0.057531	4.815568
282.099912	8000.122265	13.304883	-0.057559	4.815491
282.120063	8000.264704	13.309888	-0.057563	4.815532
282.100682	8000.279342	13.314893	-0.057560	4.815537
282.094685	8000.175597	13.319898	-0.057558	4.815506
282.102602	8000.302876	13.324903	-0.057560	4.815543
282.345260	8000.002350	13.329907	-0.057605	4.815454
282.153882	7999.981033	13.334912	-0.057569	4.815449
282.018724	8000.244857	13.339917	-0.057544	4.815527
282.127378	8000.213521	13.344922	-0.057564	4.815517
282.078407	8000.164631	13.349927	-0.057555	4.815503
282.099381	8000.244042	13.354931	-0.057559	4.815526
282.035496	8000.354111	13.359936	-0.057547	4.815559
282.230039	8000.409670	13.364941	-0.057584	4.815574
282.141222	8000.165656	13.369946	-0.057567	4.815503
282.080185	8000.330265	13.374951	-0.057556	4.815552
282.196485	8000.165493	13.379955	-0.057577	4.815503
282.164879	8000.372259	13.384960	-0.057571	4.815563
282.009989	8000.165623	13.389965	-0.057542	4.815504
282.269526	8000.207292	13.394970	-0.057591	4.815515
282.068655	8000.420886	13.399975	-0.057553	4.815578
281.983883	8000.270967	13.404979	-0.057537	4.815535
281.952677	8000.385848	13.409984	-0.057532	4.815568
282.232030	8000.215213	13.414989	-0.057584	4.815517
282.136765	8000.271341	13.419994	-0.057566	4.815534
282.022470	8000.300443	13.424999	-0.057545	4.815543
282.164929	8000.221581	13.430003	-0.057571	4.815519
282.061076	8000.388691	13.435008	-0.057552	4.815569
282.134724	8000.396313	13.440013	-0.057565	4.815571
282.449195	8000.109790	13.445018	-0.057624	4.815485
282.376886	8000.253912	13.450023	-0.057610	4.815528
282.230818	8000.221586	13.455027	-0.057583	4.815519
282.350243	8000.196839	13.460032	-0.057605	4.815511
282.218493	8000.175434	13.465037	-0.057581	4.815506
282.140406	8000.233981	13.470042	-0.057566	4.815523
282.039411	8000.280398	13.475047	-0.057547	4.815537
282.396192	8000.383506	13.480051	-0.057614	4.815566
282.222912	8000.273799	13.485056	-0.057582	4.815534
282.179981	8000.437639	13.490061	-0.057574	4.815582
282.272322	8000.269266	13.495066	-0.057591	4.815533
282.158405	8000.429800	13.500071	-0.057570	4.815580
282.284286	8000.207486	13.505075	-0.057593	4.815515
282.399037	8000.432691	13.510080	-0.057614	4.815580
282.357730	8000.230061	13.515085	-0.057606	4.815521
282.257510	8000.272216	13.520090	-0.057588	4.815534
282.217674	8000.547233	13.525095	-0.057581	4.815614
282.236731	8000.261185	13.530099	-0.057584	4.815531
282.206270	8000.365394	13.535104	-0.057578	4.815561
282.095493	8000.377457	13.540109	-0.057558	4.815565
282.225018	8000.243889	13.545114	-0.057582	4.815526
282.036729	8000.515390	13.550119	-0.057547	4.815606
282.113434	8000.353170	13.555123	-0.057561	4.815558
282.150242	8000.250130	13.560128	-0.057568	4.815528
282.174494	8000.231294	13.565133	-0.057572	4.815522
282.192662	8000.379044	13.570138	-0.057576	4.815565
282.028177	8000.286579	13.575143	-0.057545	4.815539
282.191811	8000.243326	13.580147	-0.057575	4.815526
282.330260	8000.397332	13.585152	-0.057601	4.815570
282.306976	8000.239876	13.590157	-0.057597	4.815524
282.469337	8000.133561	13.595162	-0.057627	4.815492
282.314531	8000.397066	13.600167	-0.057598	4.815570
282.293343	8000.284522	13.605171	-0.057594	4.815537
282.138701	8000.261671	13.610176	-0.057565	4.815531
282.160689	8000.403073	13.615181	-0.057569	4.815572
282.527483	8000.294783	13.620186	-0.057638	4.815539
282.295381	8000.359342	13.625191	-0.057594	4.815559
282.404784	8000.263908	13.630195	-0.057615	4.815531
282.458145	8000.266921	13.635200	-0.057625	4.815531
282.147183	8000.294921	13.640205	-0.057567	4.815541
282.342283	8000.168844	13.645210	-0.057603	4.815503
282.329732	8000.095977	13.650215	-0.057600	4.815482
282.285794	8000.105936	13.655219	-0.057592	4.815485
282.209578	8000.251063	13.660224	-0.057578	4.815528
282.327406	8000.488072	13.665229	-0.057600	4.815596
282.312362	7999.974944	13.670234	-0.057597	4.815447
282.077285	8000.260630	13.675239	-0.057553	4.815531
282.337166	8000.189045	13.680243	-0.057602	4.815509
282.383477	8000.350081	13.685248	-0.057610	4.815556
282.272565	8000.408088	13.690253	-0.057590	4.815573
282.410777	8000.285347	13.695258	-0.057615	4.815537
282.433319	8000.463089	13.700263	-0.057620	4.815589
282.289384	8000.315398	13.705267	-0.057593	4.815546
282.253196	8000.274197	13.710272	-0.057586	4.815534
282.279971	8000.200909	13.715277	-0.057591	4.815513
282.409022	8000.285307	13.720282	-0.057615	4.815537
282.132729	8000.460262	13.725287	-0.057564	4.815589
282.178040	8000.248375	13.730291	-0.057572	4.815527
282.321952	8000.435594	13.735296	-0.057599	4.815581
282.359943	8000.443697	13.740301	-0.057606	4.815583
282.370288	8000.326330	13.745306	-0.057608	4.815549
282.355825	8000.388062	13.750311	-0.057605	4.815567
282.305274	8000.318843	13.755315	-0.057596	4.815547
282.245498	8000.220623	13.760320	-0.057584	4.815519
282.233659	8000.415961	13.765325	-0.057582	4.815576
282.270650	8000.268046	13.770330	-0.057589	4.815532
282.077727	8000.388812	13.775335	-0.057553	4.815569
282.251252	8000.244216	13.780339	-0.057585	4.815526
282.508335	8000.343545	13.785344	-0.057633	4.815553
282.355908	8000.458568	13.790349	-0.057605	4.815588
282.253925	8000.285924	13.795354	-0.057586	4.815538
282.173091	8000.418153	13.800359	-0.057571	4.815577
282.226736	8000.317527	13.805363	-0.057581	4.815547
282.400816	8000.605686	13.810368	-0.057613	4.815631
282.370126	8000.416050	13.815373	-0.057607	4.815575
282.455926	8000.395023	13.820378	-0.057623	4.815569
282.503134	8000.524020	13.825383	-0.057632	4.815606
282.387263	8000.314817	13.830387	-0.057610	4.815546
282.639978	8000.524134	13.835392	-0.057658	4.815606
282.574457	8000.353158	13.840397	-0.057645	4.815556
282.434927	8000.339103	13.845402	-0.057619	4.815552
282.404671	8000.317232	13.850407	-0.057614	4.815546
282.556079	8000.249203	13.855411	-0.057642	4.815526
282.392758	8000.370457	13.860416	-0.057611	4.815562
282.480493	8000.313132	13.865421	-0.057628	4.815545
282.623282	8000.319756	13.870426	-0.057654	4.815546
282.333809	8000.360931	13.875431	-0.057600	4.815559
282.483450	8000.408271	13.880435	-0.057628	4.815572
282.793637	8000.223184	13.885440	-0.057686	4.815517
282.544384	8000.419956	13.890445	-0.057639	4.815576
282.557767	8000.190445	13.895450	-0.057642	4.815508
282.362614	8000.155174	13.900455	-0.057605	4.815499
282.624790	8000.303738	13.905459	-0.057654	4.815541
282.437091	8000.234396	13.910464	-0.057619	4.815522
282.596908	8000.473168	13.915469	-0.057649	4.815591
282.522372	8000.161001	13.920474	-0.057635	4.815500
282.529776	8000.270108	13.925479	-0.057636	4.815532
282.502884	8000.230128	13.930483	-0.057631	4.815520
282.572379	8000.256915	13.935488	-0.057644	4.815528
282.490204	8000.150846	13.940493	-0.057629	4.815497
282.733866	8000.214693	13.945498	-0.057674	4.815515
282.590351	8000.403590	13.950503	-0.057648	4.815571
282.649141	8000.284883	13.955507	-0.057659	4.815536
282.700111	8000.230158	13.960512	-0.057668	4.815519
282.677112	8000.440274	13.965517	-0.057664	4.815581
282.502956	8000.266441	13.970522	-0.057631	4.815531
282.432025	8000.436231	13.975527	-0.057618	4.815581
282.540005	8000.200799	13.980531	-0.057638	4.815512
282.604658	8000.473264	13.985536	-0.057650	4.815591
282.672662	8000.304488	13.990541	-0.057663	4.815541
282.403850	8000.153673	13.995546	-0.057613	4.815498
282.407160	8000.324685	14.000551	-0.057613	4.815548
282.525140	8000.143913	14.005555	-0.057635	4.815495
282.495338	8000.269503	14.010560	-0.057630	4.815532
282.550285	8000.238351	14.015565	-0.057640	4.815523
282.511763	8000.400127	14.020570	-0.057633	4.815570
282.374968	8000.442748	14.025575	-0.057607	4.815583
282.511904	8000.482400	14.030579	-0.057633	4.815594
282.414322	8000.354706	14.035584	-0.057614	4.815557
282.572429	8000.423556	14.040589	-0.057644	4.815577
282.436783	8000.145645	14.045594	-0.057618	4.815496
282.439285	8000.450208	14.050599	-0.057619	4.815585
282.505681	8000.411765	14.055603	-0.057631	4.815573
282.332753	8000.328775	14.060608	-0.057599	4.815550
282.234349	8000.548333	14.065613	-0.057581	4.815615
282.420212	8000.344102	14.070618	-0.057615	4.815554
282.289978	8000.406065	14.075623	-0.057591	4.815573
282.252919	8000.322109	14.080627	-0.057584	4.815548
282.463411	8000.244368	14.085632	-0.057623	4.815525
282.537573	8000.464632	14.090637	-0.057637	4.815589
282.620588	8000.116595	14.095642	-0.057652	4.815487
282.529874	8000.436719	14.100647	-0.057636	4.815581
282.552292	8000.417853	14.105651	-0.057640	4.815575
282.535880	8000.407963	14.110656	-0.057637	4.815572
282.476078	8000.406976	14.115661	-0.057626	4.815572
282.674890	8000.193342	14.120666	-0.057662	4.815509
282.496496	8000.452185	14.125671	-0.057629	4.815585
282.682072	8000.390061	14.130675	-0.057664	4.815566
282.687365	8000.331378	14.135680	-0.057665	4.815549
282.505871	8000.510033	14.140685	-0.057631	4.815602
282.662701	8000.299980	14.145690	-0.057660	4.815540
282.405091	8000.339543	14.150695	-0.057612	4.815553
282.403270	8000.434608	14.155699	-0.057612	4.815581
282.380704	8000.154286	14.160704	-0.057607	4.815499
282.378089	7999.967256	14.165709	-0.057607	4.815444
282.395920	8000.098971	14.170714	-0.057610	4.815483
282.398168	8000.371473	14.175719	-0.057611	4.815562
282.317378	8000.236577	14.180723	-0.057596	4.815523
282.505076	8000.496109	14.185728	-0.057631	4.815598
282.439511	8000.547384	14.190733	-0.057618	4.815613
282.474182	8000.426142	14.195738	-0.057625	4.815578
282.428122	8000.570699	14.200743	-0.057616	4.815620
282.551701	8000.339797	14.205747	-0.057639	4.815552
282.434135	8000.390215	14.210752	-0.057617	4.815567
282.548759	8000.337607	14.215757	-0.057639	4.815552
282.456506	8000.281591	14.220762	-0.057621	4.815536
282.396416	8000.317996	14.225767	-0.057610	4.815547
282.468721	8000.410009	14.230771	-0.057624	4.815573
282.610788	8000.338620	14.235776	-0.057650	4.815552
282.459046	8000.460065	14.240781	-0.057622	4.815588
282.772583	8000.388296	14.245786	-0.057680	4.815565
282.586250	8000.362784	14.250791	-0.057645	4.815559
282.694650	8000.291909	14.255795	-0.057665	4.815537
282.558291	7999.461589	14.260800	-0.057640	4.815296
282.490522	7996.272523	14.265805	-0.057625	4.814364
282.472766	7990.740729	14.270810	-0.057618	4.812747
282.432309	7983.947606	14.275815	-0.057606	4.810761
282.434164	7976.667170	14.280819	-0.057601	4.808631
282.433652	7969.045455	14.285824	-0.057596	4.806400
282.394709	7961.213497	14.290829	-0.057584	4.804107
282.386455	7953.378313	14.295834	-0.057577	4.801812
282.269449	7945.371657	14.300839	-0.057550	4.799466
282.330922	7937.442952	14.305843	-0.057557	4.797140
282.283600	7929.445191	14.310848	-0.057542	4.794794
282.265913	7921.385874	14.315853	-0.057534	4.792429
282.404341	7913.424200	14.320858	-0.057554	4.790090
282.278597	7905.361705	14.325863	-0.057526	4.787722
282.250942	7897.388509	14.330867	-0.057515	4.785378
281.930780	7889.438553	14.335872	-0.057451	4.783041
282.106369	7881.391156	14.340877	-0.057478	4.780673
282.179344	7873.439614	14.345882	-0.057486	4.778331
282.065756	7865.369740	14.350887	-0.057460	4.775955
282.148471	7857.404992	14.355891	-0.057470	4.773607
282.047168	7849.335915	14.360896	-0.057446	4.771229
282.033210	7841.371475	14.365901	-0.057438	4.768879
281.979760	7833.342798	14.370906	-0.057423	4.766510
282.052222	7825.395791	14.375911	-0.057431	4.764163
282.114402	7817.399730	14.380915	-0.057438	4.761801
281.831597	7809.360237	14.385920	-0.057380	4.759426
281.878089	7801.415262	14.390925	-0.057383	4.757076
281.836435	7793.369807	14.395930	-0.057370	4.754696
281.761817	7785.311164	14.400935	-0.057351	4.752311
281.790508	7777.279879	14.405939	-0.057351	4.749932
282.016444	7769.391701	14.410944	-0.057388	4.747594
281.599492	7761.258304	14.415949	-0.057305	4.745184
281.609926	7753.368356	14.420954	-0.057302	4.742844
281.429703	7745.332042	14.425959	-0.057263	4.740460
281.739018	7737.341590	14.430963	-0.057315	4.738086
281.536010	7729.325787	14.435968	-0.057272	4.735706
281.449357	7721.284776	14.440973	-0.057251	4.733316
281.480209	7713.317215	14.445978	-0.057251	4.730947
281.248875	7705.310279	14.450983	-0.057203	4.728565
281.254387	7697.277132	14.455987	-0.057199	4.726174
281.395718	7689.339406	14.460992	-0.057220	4.723810
281.299777	7681.324966	14.465997	-0.057197	4.721422
281.301959	7673.270444	14.471002	-0.057192	4.719021
281.184936	7665.350888	14.476007	-0.057165	4.716659
281.310494	7657.294040	14.481011	-0.057183	4.714255
281.032855	7649.275682	14.486016	-0.057126	4.711861
281.196015	7641.238822	14.491021	-0.057151	4.709460
281.143353	7633.299403	14.496026	-0.057136	4.707088
280.970851	7625.250400	14.501031	-0.057099	4.704681
280.863386	7617.369851	14.506035	-0.057074	4.702324
281.025804	7609.305415	14.511040	-0.057099	4.699909
280.977945	7601.281156	14.516045	-0.057084	4.697506
281.008979	7593.336553	14.521050	-0.057085	4.695126
280.815483	7585.260225	14.526055	-0.057044	4.692705
280.848753	7577.253038	14.531059	-0.057045	4.690303
280.743915	7569.310478	14.536064	-0.057020	4.687920
280.609450	7561.239813	14.541069	-0.056990	4.685497
280.981612	7553.347680	14.546074	-0.057054	4.683126
280.557685	7545.260871	14.551079	-0.056970	4.680696
280.705902	7537.369310	14.556083	-0.056992	4.678322
280.750711	7529.291337	14.561088	-0.056995	4.675892
280.473155	7521.174510	14.566093	-0.056938	4.673449
280.665561	7513.187563	14.571098	-0.056969	4.671043
280.586365	7505.186875	14.576103	-0.056949	4.668632
280.525372	7497.180084	14.581107	-0.056932	4.666218
280.397588	7489.221687	14.586112	-0.056903	4.663818
280.275603	7481.252989	14.591117	-0.056875	4.661413
280.530102	7473.257815	14.596122	-0.056917	4.658998
280.401456	7465.231255	14.601127	-0.056888	4.656574
280.153727	7457.230222	14.606131	-0.056837	4.654155
280.354854	7449.214218	14.611136	-0.056869	4.651731
280.149295	7441.201129	14.616141	-0.056825	4.649306
280.367543	7433.233676	14.621146	-0.056861	4.646894
280.092876	7425.189689	14.626151	-0.056804	4.644457
280.148483	7417.252770	14.631155	-0.056809	4.642052
280.493917	7409.212502	14.636160	-0.056869	4.639614
280.197872	7401.235769	14.641165	-0.056808	4.637194
280.266313	7393.217700	14.646170	-0.056816	4.634760
280.141126	7385.175771	14.651175	-0.056787	4.632317
279.997760	7377.185363	14.656179	-0.056755	4.629889
279.962106	7369.214739	14.661184	-0.056743	4.627466
279.794486	7361.140444	14.666189	-0.056707	4.625010
280.012689	7353.253365	14.671194	-0.056742	4.622610
279.957120	7345.171292	14.676199	-0.056727	4.620149
280.127612	7337.180727	14.681203	-0.056753	4.617714
279.922924	7329.165565	14.686208	-0.056710	4.615271
279.672885	7321.165991	14.691213	-0.056658	4.612831
279.609545	7313.141063	14.696218	-0.056641	4.610382
279.583114	7305.184821	14.701223	-0.056631	4.607953
279.517439	7297.145969	14.706227	-0.056613	4.605497
279.457983	7289.171684	14.711232	-0.056597	4.603060
279.518405	7281.146427	14.716237	-0.056603	4.600605
279.547831	7273.189737	14.721242	-0.056603	4.598171
279.341621	7265.175380	14.726247	-0.056560	4.595717
279.386190	7257.121194	14.731251	-0.056563	4.593250
279.402609	7249.130443	14.736256	-0.056561	4.590801
279.286529	7241.106549	14.741261	-0.056534	4.588341
279.380988	7233.117091	14.746266	-0.056546	4.585890
279.325259	7225.110868	14.751271	-0.056530	4.583432
279.126711	7217.130666	14.756275	-0.056488	4.580981
279.247455	7209.191545	14.761280	-0.056505	4.578542
279.313800	7201.120742	14.766285	-0.056513	4.576060
279.214908	7193.118727	14.771290	-0.056489	4.573599
278.929152	7185.084157	14.776295	-0.056430	4.571125
279.018734	7177.081135	14.781299	-0.056442	4.568661
279.089357	7169.112864	14.786304	-0.056450	4.566206
278.852605	7161.104482	14.791309	-0.056400	4.563736
278.904192	7153.156035	14.796314	-0.056405	4.561285
278.911942	7145.142254	14.801319	-0.056401	4.558811
278.834737	7137.119054	14.806323	-0.056381	4.556334
278.916400	7129.148012	14.811328	-0.056391	4.553871
278.584276	7121.060072	14.816333	-0.056324	4.551370
278.753600	7113.096305	14.821338	-0.056351	4.548908
278.607311	7105.072880	14.826343	-0.056318	4.546424
278.713248	7097.104959	14.831347	-0.056333	4.543957
278.782896	7089.101237	14.836352	-0.056340	4.541478
278.426933	7081.110369	14.841357	-0.056269	4.539000
278.601847	7073.135935	14.846362	-0.056296	4.536527
278.504727	7065.114161	14.851367	-0.056273	4.534038
278.486468	7057.061153	14.856371	-0.056264	4.531537
278.553076	7049.102471	14.861376	-0.056271	4.529065
278.355631	7041.113750	14.866381	-0.056229	4.526581
278.576427	7033.114553	14.871386	-0.056265	4.524094
278.284384	7025.117318	14.876391	-0.056206	4.521605
278.207833	7017.101979	14.881395	-0.056186	4.519109
278.352302	7009.128517	14.886400	-0.056208	4.516626
278.207669	7001.043464	14.891405	-0.056176	4.514105
278.300608	6993.017156	14.896410	-0.056188	4.511602
278.246735	6985.019470	14.901415	-0.056172	4.509107
278.020127	6976.994686	14.906419	-0.056125	4.506601
277.997262	6969.052662	14.911424	-0.056115	4.504120
277.921672	6961.039598	14.916429	-0.056096	4.501615
278.146290	6953.086250	14.921434	-0.056133	4.499128
277.984671	6945.108805	14.926439	-0.056097	4.496631
278.047179	6937.064003	14.931443	-0.056104	4.494113
277.878271	6929.050792	14.936448	-0.056067	4.491602
277.853987	6921.012859	14.941453	-0.056057	4.489083
277.889173	6913.049531	14.946458	-0.056059	4.486585
277.943177	6905.031756	14.951463	-0.056063	4.484070
277.848889	6897.053786	14.956467	-0.056041	4.481565
277.949264	6889.058421	14.961472	-0.056054	4.479053
277.742032	6881.081699	14.966477	-0.056010	4.476545
277.720368	6873.036076	14.971482	-0.056001	4.474015
277.678722	6865.018053	14.976487	-0.055988	4.471492
277.759454	6856.991315	14.981491	-0.055998	4.468965
277.667709	6849.050318	14.986496	-0.055975	4.466463
277.381855	6840.976450	14.991501	-0.055917	4.463917
277.315956	6833.054148	14.996506	-0.055900	4.461418
277.555026	6825.020902	15.001511	-0.055939	4.458884
277.482527	6817.030527	15.006515	-0.055920	4.456361
277.494715	6809.006126	15.011520	-0.055917	4.453826
277.328615	6800.976688	15.016525	-0.055881	4.451287
277.538120	6793.007309	15.021530	-0.055915	4.448767
277.446453	6785.006821	15.026535	-0.055892	4.446235
277.441479	6776.983182	15.031539	-0.055886	4.443694
277.366393	6769.050782	15.036544	-0.055867	4.441181
277.225626	6760.983994	15.041549	-0.055835	4.438623
277.142019	6753.008708	15.046554	-0.055815	4.436093
277.143790	6744.973888	15.051559	-0.055810	4.433543
277.093276	6736.952298	15.056563	-0.055795	4.430995
276.971367	6728.961910	15.061568	-0.055767	4.428456
276.989017	6720.933889	15.066573	-0.055765	4.425903
276.923893	6712.992169	15.071578	-0.055748	4.423377
276.784394	6704.982585	15.076583	-0.055717	4.420827
276.704630	6696.971885	15.081587	-0.055697	4.418275
276.863911	6688.972974	15.086592	-0.055721	4.415727
276.762019	6680.929807	15.091597	-0.055697	4.413162
276.666706	6672.938220	15.096602	-0.055674	4.410612
276.546791	6664.969290	15.101607	-0.055646	4.408067
276.772503	6656.942795	15.106611	-0.055683	4.405505
276.817825	6648.980461	15.111616	-0.055686	4.402960
276.596989	6640.960724	15.116621	-0.055640	4.400395
276.668990	6633.017952	15.121626	-0.055648	4.397854
276.748454	6624.979210	15.126631	-0.055658	4.395281
276.502373	6616.934128	15.131635	-0.055606	4.392702
276.480769	6608.961097	15.136640	-0.055597	4.390146
276.401066	6600.947996	15.141645	-0.055577	4.387576
276.323495	6592.939594	15.146650	-0.055557	4.385006
276.323068	6585.001624	15.151655	-0.055552	4.382457
276.380437	6576.942894	15.156659	-0.055558	4.379868
276.195447	6569.018563	15.161664	-0.055518	4.377320
276.152244	6560.974064	15.166669	-0.055505	4.374732
276.184855	6552.975612	15.171674	-0.055505	4.372158
276.145675	6544.919247	15.176679	-0.055493	4.369563
276.318862	6536.981834	15.181683	-0.055520	4.367007
276.373497	6528.963188	15.186688	-0.055525	4.364422
276.167425	6521.014303	15.191693	-0.055481	4.361856
276.137256	6512.988432	15.196698	-0.055470	4.359265
276.147719	6505.030326	15.201703	-0.055467	4.356695
276.121553	6496.938587	15.206707	-0.055457	4.354079
275.909695	6488.883453	15.211712	-0.055412	4.351473
275.743038	6480.878618	15.216717	-0.055376	4.348882
276.017255	6472.885977	15.221722	-0.055422	4.346296
276.024608	6464.925674	15.226727	-0.055418	4.343717
275.818162	6456.956274	15.231731	-0.055374	4.341132
275.862446	6448.983539	15.236736	-0.055377	4.338547
275.857180	6440.931011	15.241741	-0.055371	4.335933
275.695357	6432.952065	15.246746	-0.055336	4.333341
275.752336	6424.892542	15.251751	-0.055341	4.330723
275.717576	6416.898440	15.256755	-0.055329	4.328123
275.524655	6408.972130	15.261760	-0.055288	4.325543
275.495602	6400.986586	15.266765	-0.055278	4.322944
275.606982	6392.930849	15.271770	-0.055293	4.320320
275.485099	6384.962814	15.276775	-0.055265	4.317723
275.486033	6376.890597	15.281779	-0.055260	4.315090
275.594055	6368.918407	15.286784	-0.055275	4.312489
275.346117	6360.872268	15.291789	-0.055223	4.309860
275.480182	6352.907226	15.296794	-0.055243	4.307259
275.449311	6344.909790	15.301799	-0.055232	4.304645
275.368163	6336.965182	15.306803	-0.055212	4.302045
275.407593	6328.934796	15.311808	-0.055214	4.299417
275.241832	6320.958112	15.316813	-0.055178	4.296803
275.377110	6312.908541	15.321818	-0.055198	4.294166
275.298515	6304.915761	15.326823	-0.055178	4.291545
275.202145	6296.866516	15.331827	-0.055155	4.288903
275.108099	6288.902071	15.336832	-0.055132	4.286287
275.068933	6280.879401	15.341837	-0.055120	4.283652
275.281249	6272.922731	15.346842	-0.055154	4.281038
275.089319	6264.945108	15.351847	-0.055113	4.278412
274.781438	6256.892001	15.356851	-0.055050	4.275759
275.021868	6248.881934	15.361856	-0.055090	4.273123
274.933282	6240.824699	15.366861	-0.055068	4.270467
274.835585	6232.870251	15.371866	-0.055045	4.267844
274.920586	6224.896035	15.376871	-0.055055	4.265213
274.603575	6216.846691	15.381875	-0.054991	4.262553
274.605874	6208.915795	15.386880	-0.054986	4.259933
274.487209	6200.881649	15.391885	-0.054959	4.257276
274.545529	6192.895868	15.396890	-0.054964	4.254635
274.337635	6184.868594	15.401895	-0.054920	4.251977
274.275233	6176.852773	15.406899	-0.054904	4.249321
274.428281	6168.905687	15.411904	-0.054927	4.246689
274.369430	6160.878120	15.416909	-0.054911	4.244027
274.385450	6152.896776	15.421914	-0.054908	4.241379
274.342156	6144.915524	15.426919	-0.054895	4.238728
274.337901	6136.910928	15.431923	-0.054889	4.236069
274.493061	6128.914284	15.436928	-0.054913	4.233412
274.390050	6120.846591	15.441933	-0.054888	4.230728
274.096816	6112.934965	15.446938	-0.054829	4.228091
274.101655	6104.899687	15.451943	-0.054824	4.225415
274.158098	6096.918549	15.456947	-0.054829	4.222756
274.292163	6088.878341	15.461952	-0.054849	4.220076
274.174501	6080.939596	15.466957	-0.054822	4.217426
273.961298	6072.894747	15.471962	-0.054777	4.214737
273.928393	6064.909431	15.476967	-0.054766	4.212069
273.830088	6056.874252	15.481971	-0.054742	4.209382
273.834229	6048.933458	15.486976	-0.054738	4.206725
273.891428	6040.893488	15.491981	-0.054743	4.204034
273.934311	6032.939225	15.496986	-0.054746	4.201370
273.883527	6024.964999	15.501991	-0.054731	4.198697
273.797747	6016.906723	15.506995	-0.054710	4.195993
273.738360	6008.852845	15.512000	-0.054694	4.193290
273.648783	6000.786572	15.517005	-0.054672	4.190580
273.461221	5992.855943	15.522010	-0.054632	4.187913
273.567609	5984.856910	15.527015	-0.054646	4.185224
273.415712	5976.893639	15.532019	-0.054613	4.182543
273.498168	5968.905634	15.537024	-0.054623	4.179854
273.277096	5960.916053	15.542029	-0.054576	4.177160
273.347477	5952.874868	15.547034	-0.054584	4.174449
273.474267	5944.892516	15.552039	-0.054603	4.171758
273.300289	5936.853225	15.557043	-0.054565	4.169042
273.354753	5928.883627	15.562048	-0.054570	4.166351
273.261788	5920.879836	15.567053	-0.054547	4.163644
273.211487	5912.894606	15.572058	-0.054533	4.160943
273.362327	5904.919689	15.577063	-0.054556	4.158245
273.310178	5896.878554	15.582067	-0.054541	4.155521
273.244902	5888.868041	15.587072	-0.054523	4.152806
273.008277	5880.793304	15.592077	-0.054474	4.150065
273.252825	5872.864424	15.597082	-0.054514	4.147377
273.211367	5864.837612	15.602087	-0.054501	4.144651
273.192930	5856.887854	15.607091	-0.054493	4.141949
273.340098	5848.869476	15.612096	-0.054515	4.139225
273.060544	5840.881690	15.617101	-0.054457	4.136504
272.996889	5832.879595	15.622106	-0.054440	4.133779
273.033272	5824.873695	15.627111	-0.054442	4.131051
272.795519	5816.851921	15.632115	-0.054392	4.128314
272.899757	5808.860575	15.637120	-0.054406	4.125589
272.801333	5800.874611	15.642125	-0.054383	4.122862
272.852920	5792.850975	15.647130	-0.054387	4.120121
272.661941	5784.931154	15.652135	-0.054347	4.117412
272.634781	5776.869086	15.657139	-0.054336	4.114654
272.794900	5768.862857	15.662144	-0.054361	4.111915
272.650067	5760.835139	15.667149	-0.054329	4.109164
272.543776	5752.866039	15.672154	-0.054304	4.106431
272.512056	5744.863962	15.677159	-0.054292	4.103686
272.377252	5736.860298	15.682163	-0.054262	4.100938
272.538660	5728.882462	15.687168	-0.054287	4.098200
272.491309	5720.885284	15.692173	-0.054273	4.095451
272.447123	5712.867061	15.697178	-0.054259	4.092693
272.291923	5704.852259	15.702183	-0.054225	4.089933
272.266283	5696.879541	15.707187	-0.054215	4.087187
272.579307	5688.892489	15.712192	-0.054268	4.084439
272.080623	5680.929313	15.717197	-0.054170	4.081687
272.238724	5672.938307	15.722202	-0.054194	4.078932
272.186319	5664.940284	15.727207	-0.054179	4.076169
272.233527	5656.873250	15.732211	-0.054183	4.073382
272.238587	5648.879321	15.737216	-0.054179	4.070619
271.987810	5640.911145	15.742221	-0.054127	4.067858
272.284714	5632.873845	15.747226	-0.054177	4.065079
272.107417	5624.929839	15.752231	-0.054139	4.062325
272.058466	5616.903196	15.757235	-0.054124	4.059541
271.987458	5608.965759	15.762240	-0.054106	4.056786
271.937561	5600.902526	15.767245	-0.054091	4.053986
271.805335	5592.880672	15.772250	-0.054061	4.051197
271.684645	5584.908805	15.777255	-0.054034	4.048424
271.694462	5576.873261	15.782259	-0.054030	4.045628
271.765778	5568.961689	15.787264	-0.054038	4.042875
271.613878	5560.894777	15.792269	-0.054005	4.040063
271.660948	5552.934260	15.797274	-0.054008	4.037288
271.573990	5544.913393	15.802279	-0.053987	4.034489
271.314000	5536.800117	15.807283	-0.053933	4.031652
271.525010	5528.850023	15.812288	-0.053967	4.028878
271.331580	5520.844375	15.817293	-0.053926	4.026076
271.361148	5512.906895	15.822298	-0.053926	4.023300
271.330359	5504.900872	15.827303	-0.053915	4.020497
271.346900	5496.890348	15.832307	-0.053913	4.017691
271.355059	5488.901815	15.837312	-0.053909	4.014890
271.192533	5480.876640	15.842317	-0.053874	4.012072
271.187808	5472.886572	15.847322	-0.053868	4.009267
271.241541	5464.901257	15.852327	-0.053872	4.006463
271.140643	5456.873452	15.857331	-0.053848	4.003639
271.235552	5448.905477	15.862336	-0.053861	4.000837
271.037722	5440.936861	15.867341	-0.053819	3.998029
270.900458	5432.879926	15.872346	-0.053788	3.995188
270.895552	5424.904156	15.877351	-0.053782	3.992376
270.812822	5416.827910	15.882355	-0.053761	3.989525
270.883309	5408.883869	15.887360	-0.053769	3.986722
270.993435	5400.856986	15.892365	-0.053784	3.983887
270.971087	5392.901979	15.897370	-0.053775	3.981075
270.846549	5384.929169	15.902375	-0.053747	3.978252
270.514151	5376.881945	15.907379	-0.053679	3.975397
270.637829	5368.890459	15.912384	-0.053697	3.972567
270.562591	5360.859481	15.917389	-0.053678	3.969719
270.613577	5352.918013	15.922394	-0.053682	3.966902
270.570789	5344.926886	15.927399	-0.053669	3.964063
270.608305	5336.949072	15.932403	-0.053671	3.961229
270.626162	5328.974395	15.937408	-0.053669	3.958394
270.430560	5320.960506	15.942413	-0.053627	3.955539
270.435425	5312.910328	15.947418	-0.053623	3.952672
270.376256	5304.898894	15.952423	-0.053607	3.949816
270.423845	5296.895061	15.957427	-0.053610	3.946963
270.488259	5288.911917	15.962432	-0.053617	3.944115
270.333814	5280.920850	15.967437	-0.053583	3.941258
270.463367	5272.972228	15.972442	-0.053602	3.938420
270.526933	5264.984577	15.977447	-0.053609	3.935564
270.379831	5256.916435	15.982451	-0.053576	3.932673
270.410753	5248.943830	15.987456	-0.053576	3.929818
270.219493	5240.962070	15.992461	-0.053536	3.926954
270.323082	5232.939140	15.997466	-0.053550	3.924078
270.251431	5224.976147	16.002471	-0.053531	3.921218
270.001965	5216.969844	16.007475	-0.053479	3.918338
270.134253	5208.973478	16.012480	-0.053499	3.915465
270.082837	5200.955049	16.017485	-0.053484	3.912580
270.121658	5192.918849	16.022490	-0.053486	3.909687
269.959607	5184.975191	16.027495	-0.053450	3.906822
269.790327	5176.948658	16.032499	-0.053414	3.903925
270.059384	5168.985782	16.037504	-0.053459	3.901057
269.875356	5161.018621	16.042509	-0.053419	3.898176
269.919528	5152.972921	16.047514	-0.053422	3.895270
269.944415	5144.950627	16.052519	-0.053421	3.892369
269.693411	5136.927326	16.057523	-0.053369	3.889461
269.497654	5128.980455	16.062528	-0.053328	3.886579
269.456566	5120.952982	16.067533	-0.053315	3.883668
269.521272	5112.961176	16.072538	-0.053322	3.880771
269.615760	5105.023588	16.077543	-0.053334	3.877891
269.507999	5096.973016	16.082547	-0.053309	3.874965
269.540417	5088.730434	16.087552	-0.053309	3.871969
269.469378	5080.779471	16.092557	-0.053291	3.869075
269.516785	5072.864911	16.097562	-0.053295	3.866194
269.512424	5064.950496	16.102567	-0.053289	3.863310
269.440812	5056.908742	16.107571	-0.053270	3.860377
269.318695	5048.985383	16.112576	-0.053242	3.857483
269.333393	5040.932296	16.117581	-0.053240	3.854542
269.451811	5032.931704	16.122586	-0.053256	3.851621
269.252739	5024.951358	16.127591	-0.053214	3.848698
269.045797	5016.966521	16.132595	-0.053170	3.845771
269.006686	5008.995512	16.137600	-0.053158	3.842850
269.090407	5000.945372	16.142605	-0.053168	3.839901
269.067562	4993.027332	16.147610	-0.053159	3.836996
269.103407	4985.003187	16.152615	-0.053160	3.834050
268.891537	4976.989052	16.157619	-0.053115	3.831101
268.834979	4968.995265	16.162624	-0.053100	3.828161
268.846497	4960.982564	16.167629	-0.053097	3.825212
268.887201	4953.037078	16.172634	-0.053099	3.822287
268.691786	4945.029947	16.177639	-0.053057	3.819332
268.689840	4937.054329	16.182643	-0.053052	3.816390
268.921743	4929.002858	16.187648	-0.053090	3.813423
268.789001	4920.978729	16.192653	-0.053060	3.810455
268.767876	4913.018566	16.197658	-0.053050	3.807512
268.884311	4905.053161	16.202663	-0.053067	3.804567
268.595971	4897.098227	16.207667	-0.053008	3.801616
268.462133	4889.110197	16.212672	-0.052978	3.798652
268.430994	4881.069390	16.217677	-0.052967	3.795670
268.516175	4873.036444	16.222682	-0.052977	3.792690
268.378799	4865.018801	16.227687	-0.052947	3.789709
268.050197	4857.047474	16.232691	-0.052880	3.786738
268.344181	4849.066294	16.237696	-0.052930	3.783775
268.067168	4841.086103	16.242701	-0.052873	3.780798
268.009979	4833.048009	16.247706	-0.052857	3.777802
268.006260	4825.062468	16.252711	-0.052851	3.774823
267.912605	4817.046040	16.257715	-0.052828	3.771829
268.025368	4809.051889	16.262720	-0.052844	3.768846
267.941209	4801.046810	16.267725	-0.052823	3.765852
267.859992	4793.114695	16.272730	-0.052803	3.762882
267.791284	4785.096428	16.277735	-0.052785	3.759879
267.673116	4777.107637	16.282739	-0.052758	3.756883
267.810665	4769.090352	16.287744	-0.052778	3.753879
267.719835	4761.037860	16.292749	-0.052756	3.750855
267.573403	4753.070138	16.297754	-0.052723	3.747859
267.749000	4745.050605	16.302759	-0.052751	3.744848
267.648203	4737.076292	16.307763	-0.052727	3.741846
267.454897	4729.125006	16.312768	-0.052686	3.738847
267.545126	4721.109354	16.317773	-0.052697	3.735829
267.534719	4713.080843	16.322778	-0.052690	3.732801
267.595484	4705.092388	16.327783	-0.052696	3.729787
267.525398	4697.086454	16.332787	-0.052678	3.726761
267.563149	4689.123945	16.337792	-0.052680	3.723752
267.476941	4681.135362	16.342797	-0.052658	3.720728
267.390610	4673.174755	16.347802	-0.052637	3.717711
267.457509	4665.170458	16.352807	-0.052644	3.714679
267.531996	4657.026549	16.357811	-0.052653	3.711592
267.316232	4649.099701	16.362816	-0.052607	3.708578
267.298367	4641.076211	16.367821	-0.052599	3.705529
267.195060	4633.137941	16.372826	-0.052574	3.702508
267.269386	4625.137211	16.377831	-0.052583	3.699466
266.915896	4617.173476	16.382835	-0.052512	3.696424
267.083083	4609.153648	16.387840	-0.052538	3.693371
267.043607	4601.167068	16.392845	-0.052525	3.690324
266.798326	4593.170446	16.397850	-0.052474	3.687264
266.759247	4585.182447	16.402855	-0.052462	3.684211
266.808511	4577.171565	16.407859	-0.052466	3.681149
266.839920	4569.232118	16.412864	-0.052466	3.678111
266.600810	4561.208933	16.417869	-0.052417	3.675031
266.618166	4553.190066	16.422874	-0.052415	3.671957
266.732363	4545.182796	16.427879	-0.052431	3.668888
266.721791	4537.149141	16.432883	-0.052423	3.665802
266.842605	4529.212443	16.437888	-0.052441	3.662755
266.853852	4521.187506	16.442893	-0.052437	3.659668
266.541707	4513.244802	16.447898	-0.052374	3.656602
266.437419	4505.227527	16.452903	-0.052349	3.653510
266.642513	4497.170874	16.457907	-0.052382	3.650408
266.691321	4489.193135	16.462912	-0.052386	3.647330
266.479259	4481.196412	16.467917	-0.052342	3.644235
266.332703	4473.234356	16.472922	-0.052309	3.641153
266.314501	4465.277504	16.477927	-0.052300	3.638073
266.328867	4457.244572	16.482931	-0.052298	3.634963
266.283692	4449.217017	16.487936	-0.052284	3.631850
266.414270	4441.200215	16.492941	-0.052303	3.628743
266.442442	4433.212649	16.497946	-0.052303	3.625642
266.191866	4425.291585	16.502951	-0.052251	3.622557
266.110546	4417.253978	16.507955	-0.052231	3.619429
266.074876	4409.302713	16.512960	-0.052219	3.616332
265.932231	4401.278535	16.517965	-0.052187	3.613202
266.104221	4393.219093	16.522970	-0.052214	3.610063
266.077308	4385.273457	16.527975	-0.052204	3.606961
266.026645	4377.249293	16.532979	-0.052189	3.603825
266.047345	4369.300475	16.537984	-0.052188	3.600718
266.056875	4361.332202	16.542989	-0.052184	3.597600
265.776526	4353.331891	16.547994	-0.052127	3.594459
265.850823	4345.332284	16.552999	-0.052136	3.591325
265.735062	4337.299264	16.558003	-0.052109	3.588170
266.009817	4329.288019	16.563008	-0.052155	3.585032
265.769452	4321.368686	16.568013	-0.052105	3.581912
265.681617	4313.358802	16.573018	-0.052083	3.578759
265.684422	4305.395381	16.578023	-0.052078	3.575623
265.611563	4297.343125	16.583027	-0.052060	3.572448
265.641011	4289.342780	16.588032	-0.052060	3.569293
265.604788	4281.362235	16.593037	-0.052048	3.566141
265.419482	4273.393438	16.598042	-0.052008	3.562987
265.517204	4265.377728	16.603047	-0.052021	3.559820
265.313936	4257.428471	16.608051	-0.051978	3.556667
265.463654	4249.362465	16.613056	-0.052001	3.553476
265.305159	4241.308503	16.618061	-0.051966	3.550277
265.240992	4233.347605	16.623066	-0.051949	3.547116
265.204227	4225.394931	16.628071	-0.051937	3.543955
265.214940	4217.357909	16.633075	-0.051933	3.540760
265.193931	4209.386986	16.638080	-0.051924	3.537587
265.059201	4201.391857	16.643085	-0.051894	3.534398
264.854361	4193.405401	16.648090	-0.051851	3.531208
264.893157	4185.406218	16.653095	-0.051853	3.528017
264.843295	4177.392876	16.658099	-0.051838	3.524815
264.958423	4169.426564	16.663104	-0.051854	3.521633
264.853269	4161.446806	16.668109	-0.051829	3.518437
264.923850	4153.460888	16.673114	-0.051837	3.515241
265.023793	4145.431688	16.678119	-0.051851	3.512025
264.877238	4137.431895	16.683123	-0.051818	3.508811
264.751123	4129.445697	16.688128	-0.051789	3.505599
264.795162	4121.475447	16.693133	-0.051792	3.502397
264.680986	4113.491398	16.698138	-0.051766	3.499181
264.722478	4105.522785	16.703143	-0.051768	3.495973
264.542641	4097.495896	16.708147	-0.051730	3.492732
264.565321	4089.497841	16.713152	-0.051729	3.489505
264.533604	4081.517621	16.718157	-0.051718	3.486282
264.571830	4073.531589	16.723162	-0.051719	3.483055
264.459898	4065.572482	16.728167	-0.051693	3.479831
264.226929	4057.591064	16.733171	-0.051645	3.476591
264.386585	4049.559953	16.738176	-0.051669	3.473341
264.147725	4041.532526	16.743181	-0.051619	3.470076
264.165082	4033.520825	16.748186	-0.051617	3.466823
264.422113	4025.535919	16.753191	-0.051660	3.463586
264.083808	4017.559920	16.758195	-0.051592	3.460329
264.063865	4009.613595	16.763200	-0.051583	3.457093
264.113462	4001.574986	16.768205	-0.051587	3.453817
263.873834	3993.564970	16.773210	-0.051537	3.450541
263.982839	3985.604077	16.778215	-0.051552	3.447293
263.930751	3977.590391	16.783219	-0.051537	3.444015
263.834097	3969.629918	16.788224	-0.051514	3.440755
263.683757	3961.656262	16.793229	-0.051481	3.437484
263.675544	3953.622369	16.798234	-0.051474	3.434190
263.755258	3945.594337	16.803239	-0.051484	3.430898
263.592731	3937.614315	16.808243	-0.051448	3.427615
263.661597	3929.601786	16.813248	-0.051456	3.424322
263.576183	3921.671038	16.818253	-0.051435	3.421056
263.443872	3913.658604	16.823258	-0.051405	3.417750
263.689424	3905.652284	16.828263	-0.051445	3.414457
263.617545	3897.649624	16.833267	-0.051427	3.411152
263.547188	3889.675780	16.838272	-0.051408	3.407855
263.467929	3881.715713	16.843277	-0.051388	3.404560
263.543132	3873.726391	16.848282	-0.051397	3.401256
263.645432	3865.757601	16.853287	-0.051411	3.397957
263.341903	3857.756018	16.858291	-0.051349	3.394628
263.341964	3849.655769	16.863296	-0.051344	3.391265
263.170575	3841.707887	16.868301	-0.051307	3.387956
262.946773	3833.689763	16.873306	-0.051260	3.384612
263.062209	3825.747660	16.878311	-0.051276	3.381309
263.064096	3817.747277	16.883315	-0.051271	3.377975
263.149136	3809.761946	16.888320	-0.051282	3.374646
262.983796	3801.769908	16.893325	-0.051246	3.371302
262.968720	3793.765596	16.898330	-0.051238	3.367956
263.105253	3785.776422	16.903335	-0.051258	3.364617
262.877884	3777.849398	16.908339	-0.051210	3.361289
262.744062	3769.849372	16.913344	-0.051180	3.357929
263.013169	3761.812321	16.918349	-0.051225	3.354566
262.777997	3753.779189	16.923354	-0.051176	3.351182
262.848972	3745.807940	16.928359	-0.051184	3.347832
262.724478	3737.807475	16.933363	-0.051156	3.344459
262.464136	3729.884699	16.938368	-0.051102	3.341111
262.551807	3721.888656	16.943373	-0.051113	3.337741
262.511828	3713.858584	16.948378	-0.051100	3.334349
262.580961	3705.852265	16.953383	-0.051108	3.330967
262.248366	3697.884093	16.958387	-0.051041	3.327583
262.644870	3689.878569	16.963392	-0.051109	3.324207
262.538723	3681.928183	16.968397	-0.051084	3.320832
262.306545	3673.952939	16.973402	-0.051036	3.317438
262.427791	3665.952522	16.978407	-0.051053	3.314044
262.332139	3657.915635	16.983411	-0.051030	3.310622
262.427572	3649.932439	16.988416	-0.051043	3.307227
262.333902	3641.935422	16.993421	-0.051020	3.303815
262.157746	3633.956996	16.998426	-0.050982	3.300405
262.198437	3626.000405	17.003431	-0.050984	3.297008
262.030248	3618.006475	17.008435	-0.050948	3.293585
262.033750	3610.001156	17.013440	-0.050943	3.290159
262.068413	3602.015213	17.018445	-0.050944	3.286739
261.936366	3594.016945	17.023450	-0.050915	3.283304
261.919243	3586.066159	17.028455	-0.050906	3.279890
261.810614	3578.113794	17.033459	-0.050881	3.276468
261.772311	3570.091605	17.038464	-0.050868	3.273016
261.565923	3562.060581	17.043469	-0.050825	3.269549
261.662011	3554.062731	17.048474	-0.050837	3.266105
261.797958	3546.091326	17.053479	-0.050858	3.262670
261.467920	3538.088554	17.058483	-0.050791	3.259199
261.704134	3530.115418	17.063488	-0.050830	3.255761
261.575576	3522.108438	17.068493	-0.050800	3.252289
261.454210	3514.082772	17.073498	-0.050773	3.248806
261.700583	3506.103762	17.078503	-0.050813	3.245354
261.473493	3498.156790	17.083507	-0.050766	3.241893
261.526405	3490.181708	17.088512	-0.050770	3.238427
261.395529	3482.200663	17.093517	-0.050741	3.234948
261.237280	3474.136293	17.098522	-0.050706	3.231428
261.360504	3466.139671	17.103527	-0.050724	3.227945
261.122295	3458.136090	17.108531	-0.050674	3.224440
261.135874	3450.193416	17.113536	-0.050671	3.220968
261.157162	3442.203679	17.118541	-0.050670	3.217473
261.075360	3434.206669	17.123546	-0.050650	3.213966
261.026005	3426.228181	17.128551	-0.050635	3.210464
260.988696	3418.235968	17.133555	-0.050623	3.206954
260.887690	3410.284109	17.138560	-0.050599	3.203454
260.805687	3402.299481	17.143565	-0.050579	3.199937
260.805705	3394.316593	17.148570	-0.050573	3.196421
260.807101	3386.299203	17.153575	-0.050568	3.192885
260.627387	3378.274750	17.158579	-0.050530	3.189335
260.774429	3370.299403	17.163584	-0.050552	3.185816
260.627838	3362.347515	17.168589	-0.050519	3.182291
260.663002	3354.330723	17.173594	-0.050521	3.178741
260.749934	3346.358705	17.178599	-0.050532	3.175210
260.615976	3338.345106	17.183603	-0.050501	3.171646
260.439943	3330.391681	17.188608	-0.050463	3.168104
260.361941	3322.409010	17.193613	-0.050444	3.164548
260.244612	3314.434960	17.198618	-0.050417	3.160991
260.413266	3306.460368	17.203623	-0.050443	3.157442
260.229642	3298.445074	17.208627	-0.050403	3.153856
260.247878	3290.414425	17.213632	-0.050401	3.150267
260.161717	3282.457507	17.218637	-0.050380	3.146702
259.965087	3274.460566	17.223642	-0.050338	3.143111
260.123298	3266.475633	17.228647	-0.050363	3.139537
260.046880	3258.497062	17.233651	-0.050343	3.135951
259.871234	3250.530487	17.238656	-0.050305	3.132362
259.986643	3242.506289	17.243661	-0.050321	3.128756
259.939846	3234.508014	17.248666	-0.050307	3.125150
260.224820	3226.540783	17.253671	-0.050355	3.121568
259.952830	3218.585313	17.258675	-0.050299	3.117963
259.832163	3210.599296	17.263680	-0.050272	3.114347
259.957881	3202.593938	17.268685	-0.050290	3.110729
259.820358	3194.603452	17.273690	-0.050259	3.107102
259.744710	3186.644376	17.278695	-0.050240	3.103487
259.586366	3178.636960	17.283699	-0.050205	3.099842
259.650538	3170.663358	17.288704	-0.050212	3.096219
259.530257	3162.671700	17.293709	-0.050184	3.092575
259.474017	3154.661854	17.298714	-0.050168	3.088921
259.515376	3146.686528	17.303719	-0.050171	3.085283
259.603797	3138.685786	17.308723	-0.050182	3.081631
259.487160	3130.738457	17.313728	-0.050155	3.077990
259.518278	3122.732455	17.318733	-0.050156	3.074324
259.113512	3114.672833	17.323738	-0.050075	3.070609
259.162865	3106.711438	17.328743	-0.050079	3.066956
259.175543	3098.726598	17.333747	-0.050076	3.063286
259.215978	3090.723399	17.338752	-0.050079	3.059605
259.220649	3082.803225	17.343757	-0.050074	3.055955
259.046400	3074.796590	17.348762	-0.050037	3.052253
259.330156	3066.803295	17.353767	-0.050084	3.048575
259.339066	3058.817478	17.358771	-0.050081	3.044882
258.952035	3050.893023	17.363776	-0.050003	3.041194
259.145057	3042.902205	17.368781	-0.050034	3.037499
259.106185	3034.885227	17.373786	-0.050022	3.033776
258.861218	3026.903546	17.378791	-0.049971	3.030055
258.793672	3018.912666	17.383795	-0.049953	3.026334
258.908891	3010.928003	17.388800	-0.049969	3.022619
258.903037	3002.961059	17.393805	-0.049963	3.018903
258.705969	2994.991871	17.398810	-0.049921	3.015171
258.795729	2986.967887	17.403815	-0.049932	3.011424
258.661868	2978.993992	17.408819	-0.049902	3.007684
258.570935	2971.008264	17.413824	-0.049880	3.003936
258.657570	2963.046408	17.418829	-0.049891	3.000203
258.427633	2955.111912	17.423834	-0.049843	2.996463
258.510166	2947.079458	17.428839	-0.049853	2.992688
258.181397	2939.073539	17.433843	-0.049787	2.988900
258.365100	2931.073134	17.438848	-0.049816	2.985135
258.295213	2923.137448	17.443853	-0.049797	2.981383
258.058015	2915.159025	17.448858	-0.049748	2.977598
258.225503	2907.158212	17.453863	-0.049774	2.973818
258.151570	2899.136055	17.458867	-0.049755	2.970010
258.066744	2891.194399	17.463872	-0.049734	2.966236
258.119697	2883.222511	17.468877	-0.049739	2.962449
258.124268	2875.226003	17.473882	-0.049734	2.958644
258.177281	2867.259444	17.478887	-0.049739	2.954850
258.125239	2859.232696	17.483891	-0.049724	2.951017
258.030922	2851.263420	17.488896	-0.049701	2.947204
257.840859	2843.291399	17.493901	-0.049660	2.943380
257.731141	2835.313306	17.498906	-0.049635	2.939553
258.009172	2827.346450	17.503911	-0.049681	2.935746
257.754745	2819.343171	17.508915	-0.049629	2.931889
257.572671	2811.364077	17.513920	-0.049590	2.928042
257.682698	2803.395395	17.518925	-0.049605	2.924210
257.692502	2795.393721	17.523930	-0.049601	2.920352
257.832599	2787.449070	17.528935	-0.049622	2.916524
257.557139	2779.414580	17.533939	-0.049566	2.912625
257.629287	2771.384970	17.538944	-0.049574	2.908741
257.503694	2763.436756	17.543949	-0.049545	2.904881
257.352851	2755.471752	17.548954	-0.049512	2.901007
257.318126	2747.520031	17.553959	-0.049500	2.897140
257.321628	2739.507403	17.558963	-0.049496	2.893240
257.176548	2731.520149	17.563968	-0.049464	2.889340
257.327707	2723.544062	17.568973	-0.049486	2.885455
257.341359	2715.580544	17.573978	-0.049484	2.881564
257.274013	2707.629800	17.578983	-0.049466	2.877670
257.121842	2699.640125	17.583987	-0.049432	2.873747
256.983640	2691.626817	17.588992	-0.049402	2.869807
257.312777	2683.639475	17.593997	-0.049458	2.865900
257.161767	2675.669870	17.599002	-0.049424	2.861971
257.282467	2667.698443	17.604007	-0.049441	2.858050
257.102836	2659.717369	17.609011	-0.049403	2.854102
256.910892	2651.758928	17.614016	-0.049362	2.850159
256.798388	2643.820903	17.619021	-0.049336	2.846226
256.942227	2635.788043	17.624026	-0.049357	2.842254
257.025460	2627.839867	17.629031	-0.049368	2.838315
256.861484	2619.869875	17.634035	-0.049332	2.834346
256.835168	2611.820838	17.639040	-0.049322	2.830340
256.814306	2603.875262	17.644045	-0.049313	2.826380
256.643968	2595.904140	17.649050	-0.049276	2.822393
256.614673	2587.950082	17.654055	-0.049265	2.818417
256.712540	2579.960259	17.659059	-0.049278	2.814425
256.346986	2571.977664	17.664064	-0.049205	2.810404
256.239718	2564.003091	17.669069	-0.049179	2.806397
256.198794	2556.011213	17.674074	-0.049167	2.802378
256.210378	2548.061955	17.679079	-0.049164	2.798379
256.088429	2540.075732	17.684083	-0.049136	2.794347
256.029042	2532.066656	17.689088	-0.049119	2.790301
255.996535	2524.109935	17.694093	-0.049108	2.786278
255.922064	2516.121523	17.699098	-0.049089	2.782230
255.874421	2508.192738	17.704103	-0.049075	2.778209
255.798515	2500.187797	17.709107	-0.049055	2.774141
255.818894	2492.173575	17.714112	-0.049054	2.770068
255.802514	2484.204841	17.719117	-0.049046	2.766010
255.876307	2476.229288	17.724122	-0.049054	2.761948
255.903114	2468.272163	17.729127	-0.049054	2.757886
255.576652	2460.310928	17.734131	-0.048988	2.753796
255.372928	2452.244914	17.739136	-0.048945	2.749652
255.737546	2444.270112	17.744141	-0.049008	2.745584
255.498775	2436.329622	17.749146	-0.048958	2.741491
255.301277	2428.385931	17.754151	-0.048916	2.737392
255.383518	2420.376888	17.759155	-0.048926	2.733271
255.299892	2412.384454	17.764160	-0.048905	2.729142
255.383139	2404.439856	17.769165	-0.048915	2.725041
255.260764	2396.478011	17.774170	-0.048887	2.720913
255.234878	2388.530649	17.779175	-0.048877	2.716792
255.091545	2380.538482	17.784179	-0.048845	2.712634
255.058505	2372.539448	17.789184	-0.048834	2.708473
255.087895	2364.585378	17.794189	-0.048834	2.704333
255.024109	2356.605607	17.799194	-0.048817	2.700167
254.906962	2348.676853	17.804199	-0.048790	2.696018
254.887785	2340.661506	17.809203	-0.048781	2.691824
254.925119	2332.653629	17.814208	-0.048783	2.687631
254.877854	2324.729083	17.819213	-0.048769	2.683469
254.744140	2316.750753	17.824218	-0.048739	2.679267
255.014161	2308.766886	17.829223	-0.048784	2.675081
255.062309	2300.745379	17.834227	-0.048788	2.670855
254.862687	2292.772577	17.839232	-0.048745	2.666632
254.882656	2284.830595	17.844237	-0.048744	2.662433
254.834564	2276.865267	17.849242	-0.048730	2.658210
254.863797	2268.903762	17.854247	-0.048730	2.653987
254.578238	2260.910374	17.859251	-0.048672	2.649721
254.556353	2252.942829	17.864256	-0.048662	2.645478
254.501067	2245.019382	17.869261	-0.048647	2.641250
254.322069	2237.052305	17.874266	-0.048608	2.636983
254.291493	2229.067697	17.879271	-0.048597	2.632711
254.340040	2221.059816	17.884275	-0.048601	2.628423
254.243677	2213.091007	17.889280	-0.048578	2.624141
254.376328	2205.125786	17.894285	-0.048597	2.619868
254.288342	2197.173877	17.899290	-0.048576	2.615581
254.102044	2189.203872	17.904295	-0.048536	2.611270
254.229007	2181.209638	17.909299	-0.048554	2.606961
254.227539	2173.232138	17.914304	-0.048549	2.602644
254.223755	2165.302405	17.919309	-0.048543	2.598346
254.119939	2157.292553	17.924314	-0.048518	2.593991
254.132395	2149.161779	17.929319	-0.048515	2.589570
253.932134	2141.236449	17.934323	-0.048473	2.585240
253.887049	2133.310477	17.939328	-0.048459	2.580912
253.898190	2125.390756	17.944333	-0.048456	2.576584
254.026358	2117.381286	17.949338	-0.048475	2.572208
253.930647	2109.436052	17.954343	-0.048452	2.567844
253.640659	2101.502779	17.959347	-0.048393	2.563466
253.852909	2093.527386	17.964352	-0.048427	2.559092
253.835219	2085.581312	17.969357	-0.048418	2.554711
253.525628	2077.590137	17.974362	-0.048356	2.550277
253.545956	2069.635430	17.979367	-0.048354	2.545878
253.548010	2061.677075	17.984371	-0.048349	2.541469
253.406920	2053.732776	17.989376	-0.048318	2.537049
253.520094	2045.755656	17.994381	-0.048334	2.532622
253.394844	2037.769394	17.999386	-0.048305	2.528164
253.275255	2029.827030	18.004391	-0.048278	2.523724
253.280604	2021.870422	18.009395	-0.048273	2.519277
253.164689	2013.904148	18.014400	-0.048247	2.514808
253.197935	2005.903733	18.019405	-0.048248	2.510322
253.059485	1997.931092	18.024410	-0.048217	2.505832
253.058080	1989.973158	18.029415	-0.048211	2.501352
253.057576	1982.019683	18.034419	-0.048206	2.496866
253.100674	1974.033726	18.039424	-0.048209	2.492357
253.069222	1966.082589	18.044429	-0.048198	2.487854
252.944870	1958.131506	18.049434	-0.048169	2.483336
252.988038	1950.178145	18.054439	-0.048172	2.478821
252.708762	1942.245836	18.059443	-0.048115	2.474286
252.767095	1934.218610	18.064448	-0.048120	2.469713
252.896008	1926.265799	18.069453	-0.048139	2.465180
252.633489	1918.321446	18.074458	-0.048085	2.460614
252.726435	1910.367788	18.079463	-0.048097	2.456061
252.674195	1902.390010	18.084467	-0.048082	2.451474
252.545055	1894.422104	18.089472	-0.048053	2.446879
252.444630	1886.491433	18.094477	-0.048029	2.442299
252.433022	1878.536467	18.099482	-0.048022	2.437702
252.588106	1870.531688	18.104487	-0.048045	2.433081
252.348721	1862.542176	18.109491	-0.047996	2.428430
252.354511	1854.564426	18.114496	-0.047991	2.423796
252.341103	1846.637417	18.119501	-0.047984	2.419180
252.036490	1838.698363	18.124506	-0.047922	2.414527
252.078990	1830.718839	18.129511	-0.047924	2.409867
252.240931	1822.738564	18.134515	-0.047949	2.405208
251.672575	1814.860786	18.139520	-0.047838	2.400542
251.780332	1806.911966	18.144525	-0.047853	2.395879
251.764998	1798.891707	18.149530	-0.047845	2.391154
251.838669	1790.928518	18.154535	-0.047854	2.386461
251.750727	1782.978841	18.159539	-0.047832	2.381754
251.850895	1775.005220	18.164544	-0.047846	2.377039
251.944432	1767.054806	18.169549	-0.047858	2.372327
251.566560	1759.125841	18.174554	-0.047782	2.367581
251.685870	1751.162265	18.179559	-0.047799	2.362845
251.738359	1743.210526	18.184563	-0.047804	2.358100
251.502030	1735.261115	18.189568	-0.047755	2.353325
251.460224	1727.281386	18.194573	-0.047742	2.348537
251.299651	1719.327027	18.199578	-0.047706	2.343745
251.599466	1711.341341	18.204583	-0.047757	2.338961
251.452684	1703.421337	18.209587	-0.047724	2.334171
251.215915	1695.462851	18.214592	-0.047675	2.329341
251.408012	1687.489622	18.219597	-0.047706	2.324527
251.335785	1679.555988	18.224602	-0.047687	2.319705
251.169896	1671.638610	18.229607	-0.047651	2.314875
251.238756	1663.642809	18.234611	-0.047659	2.310007
251.096484	1655.691711	18.239616	-0.047627	2.305138
251.016776	1647.784829	18.244621	-0.047607	2.300291
250.967043	1639.817075	18.249626	-0.047592	2.295399
251.032912	1631.830131	18.254631	-0.047599	2.290494
250.890621	1623.899547	18.259635	-0.047568	2.285596
250.641197	1615.978602	18.264640	-0.047516	2.280685
250.949469	1608.016980	18.269645	-0.047568	2.275785
250.547338	1600.020189	18.274650	-0.047488	2.270792
250.609595	1592.039641	18.279655	-0.047495	2.265838
250.617445	1584.094554	18.284659	-0.047491	2.260890
250.458297	1576.167308	18.289664	-0.047456	2.255928
250.404181	1568.231769	18.294669	-0.047441	2.250959
250.436000	1560.242362	18.299674	-0.047441	2.245953
250.505818	1552.317048	18.304679	-0.047449	2.240980
250.272545	1544.415209	18.309683	-0.047401	2.235983
250.190520	1536.436897	18.314688	-0.047380	2.230940
250.385881	1528.466403	18.319693	-0.047411	2.225915
250.335419	1520.519709	18.324698	-0.047397	2.220873
250.261649	1512.600739	18.329703	-0.047378	2.215834
250.030399	1504.667132	18.334707	-0.047330	2.210760
249.901029	1496.712379	18.339712	-0.047300	2.205670
250.142260	1488.780571	18.344717	-0.047340	2.200617
249.792109	1480.865470	18.349722	-0.047270	2.195509
249.801318	1472.876482	18.354727	-0.047266	2.190374
249.850808	1464.913324	18.359731	-0.047270	2.185248
249.646708	1456.999693	18.364736	-0.047227	2.180118
249.791038	1449.058471	18.369741	-0.047249	2.174990
249.648288	1441.094264	18.374746	-0.047217	2.169809
249.705414	1433.149950	18.379751	-0.047222	2.164647
249.542112	1425.249499	18.384755	-0.047187	2.159480
249.566599	1417.296399	18.389760	-0.047186	2.154284
249.579328	1409.342238	18.394765	-0.047183	2.149074
249.473905	1401.386981	18.399770	-0.047158	2.143840
249.458208	1393.477900	18.404775	-0.047150	2.138631
249.280976	1385.552680	18.409779	-0.047112	2.133384
249.214909	1377.603286	18.414784	-0.047094	2.128118
249.262648	1369.668736	18.419789	-0.047098	2.122860
249.146322	1361.737573	18.424794	-0.047071	2.117575
249.114566	1353.768228	18.429799	-0.047060	2.112260
249.206717	1345.779812	18.434803	-0.047072	2.106931
249.001484	1337.875491	18.439808	-0.047029	2.101615
249.105470	1329.941162	18.444813	-0.047043	2.096296
248.930332	1322.009019	18.449818	-0.047005	2.090938
248.898632	1314.083644	18.454823	-0.046994	2.085585
248.745163	1306.180438	18.459827	-0.046960	2.080220
248.528084	1298.277571	18.464832	-0.046915	2.074836
248.701338	1290.298565	18.469837	-0.046942	2.069425
248.600854	1282.361965	18.474842	-0.046918	2.064001
248.482394	1274.456432	18.479847	-0.046890	2.058582
248.317626	1266.547872	18.484851	-0.046855	2.053143
248.467626	1258.566163	18.489856	-0.046877	2.047670
248.384801	1250.666512	18.494861	-0.046857	2.042215
248.212797	1242.774504	18.499866	-0.046820	2.036742
248.361951	1234.787279	18.504871	-0.046842	2.031221
248.228963	1226.863432	18.509875	-0.046812	2.025701
248.062661	1218.951642	18.514880	-0.046776	2.020170
248.190096	1211.024470	18.519885	-0.046795	2.014643
248.113096	1203.077540	18.524890	-0.046775	2.009066
248.072094	1195.160245	18.529895	-0.046762	2.003498
248.098483	1187.255189	18.534899	-0.046762	1.997931
247.828031	1179.346720	18.539904	-0.046706	1.992314
247.812514	1171.408533	18.544909	-0.046698	1.986687
247.704425	1163.489057	18.549914	-0.046673	1.981048
247.743155	1155.568770	18.554919	-0.046675	1.975407
247.889654	1147.621371	18.559923	-0.046697	1.969743
247.569022	1139.738241	18.564928	-0.046632	1.964058
247.764098	1131.819629	18.569933	-0.046663	1.958386
247.628235	1123.878666	18.574938	-0.046633	1.952646
247.506358	1115.931658	18.579943	-0.046605	1.946887
247.646543	1107.999384	18.584947	-0.046626	1.941149
247.595760	1100.084429	18.589952	-0.046611	1.935387
247.607815	1092.180389	18.594957	-0.046608	1.929622
247.271485	1084.299006	18.599962	-0.046540	1.923817
247.245512	1076.406472	18.604967	-0.046530	1.918022
247.277976	1068.472419	18.609971	-0.046531	1.912184
247.018147	1060.560138	18.614976	-0.046478	1.906312
246.961437	1052.676982	18.619981	-0.046462	1.900467
246.829406	1044.771632	18.624986	-0.046432	1.894578
246.755232	1036.848271	18.629991	-0.046413	1.888664
246.606842	1028.953543	18.634995	-0.046380	1.882744
246.629132	1021.044644	18.640000	-0.046379	1.876815
246.840262	1013.089830	18.645005	-0.046414	1.870854
246.657608	1005.186843	18.650010	-0.046374	1.864867
246.573771	997.307004	18.655015	-0.046354	1.858891
246.535667	989.392409	18.660019	-0.046341	1.852873
246.512067	981.473078	18.665024	-0.046332	1.846835
246.456291	973.592721	18.670029	-0.046316	1.840802
246.397475	965.704954	18.675034	-0.046300	1.834744
246.368254	957.782212	18.680039	-0.046289	1.828642
246.244507	949.897840	18.685043	-0.046261	1.822538
246.250146	941.993045	18.690048	-0.046257	1.816413
246.318392	934.082950	18.695053	-0.046265	1.810271
246.108231	926.209492	18.700058	-0.046220	1.804103
246.240348	918.306929	18.705063	-0.046240	1.797932
246.053842	910.403957	18.710067	-0.046200	1.791701
245.863855	902.492574	18.715072	-0.046159	1.785441
245.756078	894.633915	18.720077	-0.046134	1.779211
245.770758	886.728430	18.725082	-0.046132	1.772937
245.635528	878.846252	18.730087	-0.046101	1.766640
245.604683	870.968373	18.735091	-0.046090	1.760338
245.744408	863.055349	18.740096	-0.046111	1.754006
245.669855	855.180230	18.745101	-0.046092	1.747654
245.497212	847.306126	18.750106	-0.046055	1.741268
245.455689	839.432790	18.755111	-0.046042	1.734876
245.684499	831.516762	18.760115	-0.046079	1.728459
245.327023	823.681171	18.765120	-0.046008	1.722009
245.495117	815.791606	18.770125	-0.046034	1.715559
245.299733	807.910221	18.775130	-0.045992	1.709044
245.305160	800.028681	18.780135	-0.045988	1.702529
245.077563	792.196572	18.785139	-0.045941	1.696001
244.882171	784.317504	18.790144	-0.045899	1.689412
244.954456	776.435892	18.795149	-0.045907	1.682830
244.756420	768.593855	18.800154	-0.045865	1.676220
244.911379	760.676988	18.805159	-0.045889	1.669568
244.931708	752.804186	18.810163	-0.045888	1.662908
244.668686	744.981127	18.815168	-0.045834	1.656226
244.676967	737.115062	18.820173	-0.045830	1.649517
244.606678	729.249077	18.825178	-0.045812	1.642769
244.666430	721.393034	18.830183	-0.045818	1.636020
244.537828	713.496027	18.835187	-0.045789	1.629182
244.355353	705.639065	18.840192	-0.045750	1.622342
244.433528	697.781306	18.845197	-0.045759	1.615509
244.291127	689.934488	18.850202	-0.045727	1.608626
244.183626	682.093926	18.855207	-0.045702	1.601723
244.262340	674.247036	18.860211	-0.045712	1.594811
244.259428	666.367512	18.865216	-0.045706	1.587829
244.153960	658.545049	18.870221	-0.045681	1.580851
243.983625	650.730163	18.875226	-0.045644	1.573841
244.088729	642.858379	18.880231	-0.045659	1.566787
243.890855	635.067203	18.885235	-0.045617	1.559731
243.501698	627.270887	18.890240	-0.045539	1.552609
243.640258	619.383776	18.895245	-0.045560	1.545450
243.519453	611.564494	18.900250	-0.045532	1.538281
243.492752	603.715413	18.905255	-0.045522	1.531064
243.477124	595.891357	18.910259	-0.045514	1.523839
243.518919	588.053356	18.915264	-0.045517	1.516575
243.325072	580.249242	18.920269	-0.045476	1.509272
243.231000	572.427018	18.925274	-0.045453	1.501931
243.301362	564.600801	18.930279	-0.045461	1.494576
243.201766	556.792329	18.935283	-0.045437	1.487175
243.172564	548.984030	18.940288	-0.045427	1.479748
243.208343	541.150920	18.945293	-0.045428	1.472270
242.762493	533.369709	18.950298	-0.045340	1.464728
242.735027	525.567044	18.955303	-0.045330	1.457192
242.733146	517.752319	18.960307	-0.045324	1.449609
242.596270	509.966132	18.965312	-0.045294	1.441993
242.532264	502.184039	18.970317	-0.045277	1.434352
242.552075	494.361955	18.975322	-0.045275	1.426644
242.532694	486.577170	18.980327	-0.045267	1.418925
242.435363	478.802875	18.985331	-0.045243	1.411162
242.289151	471.026959	18.990336	-0.045211	1.403345
242.408175	463.242417	18.995341	-0.045228	1.395521
242.224444	455.459661	19.000346	-0.045189	1.387603
242.044314	447.711222	19.005351	-0.045150	1.379675
242.018391	439.939253	19.010355	-0.045140	1.371704
241.950231	432.168679	19.015360	-0.045123	1.363680
241.866682	424.423703	19.020365	-0.045102	1.355633
241.588870	416.686869	19.025370	-0.045045	1.347512
241.772389	408.888895	19.030375	-0.045074	1.339358
241.651379	401.158164	19.035379	-0.045047	1.331172
241.442121	393.430848	19.040384	-0.045003	1.322923
241.484767	385.671355	19.045389	-0.045005	1.314633
241.354398	377.822780	19.050394	-0.044976	1.306163
241.317389	370.104253	19.055399	-0.044964	1.297796
241.247084	362.385190	19.060403	-0.044946	1.289368
241.139949	354.672475	19.065408	-0.044921	1.280884
241.038406	346.985887	19.070413	-0.044897	1.272374
240.987623	339.265821	19.075418	-0.044882	1.263779
240.851018	331.581762	19.080423	-0.044852	1.255149
240.959098	323.855159	19.085427	-0.044867	1.246458
240.718103	316.205798	19.090432	-0.044817	1.237726
240.595829	308.514356	19.095437	-0.044789	1.228907
240.417909	300.838135	19.100442	-0.044751	1.220031
240.280881	293.170151	19.105447	-0.044721	1.211108
240.317519	285.488094	19.110451	-0.044722	1.202137
240.168618	277.836993	19.115456	-0.044690	1.193097
240.235219	270.149494	19.120461	-0.044697	1.183988
239.992944	262.536725	19.125466	-0.044647	1.174836
239.896859	254.885064	19.130471	-0.044624	1.165594
240.103251	247.228700	19.135475	-0.044658	1.156336
239.840790	239.582056	19.140480	-0.044604	1.146917
239.811654	231.964791	19.145485	-0.044593	1.137505
239.690260	224.351146	19.150490	-0.044566	1.128000
239.387702	216.783285	19.155495	-0.044504	1.118432
239.331191	209.187390	19.160499	-0.044489	1.108800
239.190762	201.600591	19.165504	-0.044458	1.099077
239.237728	194.006819	19.170509	-0.044462	1.089299
239.051434	186.454936	19.175514	-0.044422	1.079435
238.911002	178.899034	19.180519	-0.044391	1.069485
238.881107	171.341216	19.185523	-0.044380	1.059464
238.688119	163.815765	19.190528	-0.044339	1.049353
238.563152	156.302323	19.195533	-0.044311	1.039177
238.693780	148.742709	19.200538	-0.044331	1.028896
238.342771	141.282477	19.205543	-0.044260	1.018534
238.142496	133.810501	19.210547	-0.044218	1.008086
238.148386	126.313236	19.215552	-0.044214	0.997543
238.173816	118.787019	19.220557	-0.044214	0.986850
237.726983	111.398804	19.225562	-0.044126	0.976121
237.567679	103.957686	19.230567	-0.044092	0.965269
237.709920	96.501195	19.235571	-0.044113	0.954348
237.484048	89.096863	19.240576	-0.044066	0.943282
237.383149	81.713143	19.245581	-0.044043	0.932150
237.005230	74.381385	19.250586	-0.043967	0.920888
236.655441	67.051562	19.255591	-0.043898	0.909497
236.483574	59.943718	19.260595	-0.043861	0.898358