Fri Mar 12 11:49:27 2021


Number of Points = 3624

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.982485	0.008617	0.000000	0.000020	0.720866
1.055521	-0.010499	0.005005	0.000006	0.720854
0.966230	-0.158806	0.010010	0.000023	0.720531
1.155672	-0.186439	0.015014	-0.000012	0.720543
1.124224	-0.182427	0.020019	-0.000006	0.720540
0.889225	-0.143038	0.025024	0.000038	0.720535
1.111985	-0.179142	0.030029	-0.000004	0.720542
1.030261	-0.168951	0.035034	0.000012	0.720533
0.977889	-0.154354	0.040038	0.000021	0.720543
1.091974	-0.177963	0.045043	0.000000	0.720537
1.186751	-0.194963	0.050048	-0.000017	0.720537
1.154527	-0.186491	0.055053	-0.000011	0.720542
0.980357	-0.161106	0.060058	0.000021	0.720531
1.093657	-0.175537	0.065062	-0.000000	0.720542
0.890353	-0.140167	0.070067	0.000038	0.720540
0.983659	-0.157221	0.075072	0.000021	0.720539
1.088612	-0.299903	0.080077	0.000001	0.720295
1.054123	-0.331808	0.085082	0.000008	0.720220
1.091926	-0.333153	0.090086	0.000001	0.720231
0.978139	-0.315031	0.095091	0.000022	0.720226
1.096058	-0.338450	0.100096	-0.000000	0.720221
1.112864	-0.337205	0.105101	-0.000003	0.720230
0.975286	-0.380940	0.110106	0.000022	0.720095
1.005103	-0.482716	0.115110	0.000017	0.719905
0.929045	-0.471866	0.120115	0.000031	0.719900
0.934911	-0.473943	0.125120	0.000030	0.719898
1.079245	-0.493787	0.130125	0.000003	0.719909
1.221920	-0.580115	0.135130	-0.000023	0.719789
1.155466	-0.662013	0.140134	-0.000011	0.719604
1.079766	-0.649682	0.145139	0.000003	0.719602
1.097281	-0.653674	0.150144	0.000000	0.719600
1.192574	-0.713208	0.155149	-0.000017	0.719516
0.964614	-0.798799	0.160154	0.000025	0.719267
1.046620	-0.809409	0.165158	0.000010	0.719275
0.914388	-0.788988	0.170163	0.000035	0.719269
0.864495	-0.862372	0.175168	0.000044	0.719106
0.954045	-0.949495	0.180173	0.000027	0.718966
0.893983	-0.943983	0.185178	0.000039	0.718956
0.980958	-0.971896	0.190182	0.000022	0.718931
0.888724	-1.101762	0.195187	0.000040	0.718642
1.051994	-1.131317	0.200192	0.000009	0.718641
1.137231	-1.144365	0.205197	-0.000006	0.718645
0.990116	-1.269141	0.210202	0.000021	0.718347
0.933245	-1.256603	0.215206	0.000032	0.718352
0.875950	-1.267071	0.220211	0.000042	0.718311
0.926248	-1.428004	0.225216	0.000033	0.718011
0.700211	-1.384388	0.230221	0.000075	0.718017
0.880579	-1.472057	0.235226	0.000042	0.717907
0.875057	-1.575460	0.240230	0.000043	0.717701
0.700598	-1.545020	0.245235	0.000075	0.717700
0.703167	-1.662308	0.250240	0.000075	0.717469
0.751732	-1.715407	0.255245	0.000066	0.717381
0.572730	-1.712062	0.260250	0.000099	0.717324
0.588187	-1.836200	0.265254	0.000097	0.717084
0.451598	-1.813371	0.270259	0.000122	0.717081
0.387971	-1.917820	0.275264	0.000134	0.716852
0.452917	-1.976757	0.280269	0.000122	0.716758
0.528463	-2.042820	0.285274	0.000108	0.716654
0.436466	-2.130242	0.290278	0.000125	0.716448
0.251203	-2.098859	0.295283	0.000160	0.716445
0.169677	-2.240995	0.300288	0.000175	0.716135
0.264202	-2.257008	0.305293	0.000158	0.716136
-0.524649	-2.208439	0.310298	0.000305	0.715954
-1.356802	-2.095259	0.315302	0.000459	0.715884
-1.468140	-2.077830	0.320307	0.000480	0.715880
-1.894998	-2.172490	0.325312	0.000560	0.715541
-1.924900	-2.163977	0.330317	0.000565	0.715547
-2.666208	-2.037471	0.335322	0.000703	0.715536
-2.914207	-2.148166	0.340326	0.000750	0.715229
-3.211112	-2.094764	0.345331	0.000805	0.715230
-3.586873	-2.029596	0.350336	0.000875	0.715227
-3.464621	-2.134629	0.355341	0.000852	0.715061
-4.398180	-2.048835	0.360346	0.001026	0.714901
-3.906420	-2.134163	0.365350	0.000935	0.714906
-4.263579	-2.071166	0.370355	0.001001	0.714905
-4.849598	-2.066927	0.375360	0.001110	0.714706
-4.770399	-2.129004	0.380365	0.001096	0.714610
-4.894172	-2.110415	0.385370	0.001119	0.714603
-5.208770	-2.051657	0.390374	0.001177	0.714609
-5.112047	-2.138114	0.395379	0.001159	0.714471
-5.934826	-2.091982	0.400384	0.001313	0.714272
-5.748951	-2.122230	0.405389	0.001278	0.714277
-6.309481	-2.027320	0.410394	0.001382	0.714267
-6.031037	-2.074571	0.415398	0.001331	0.714272
-6.315437	-2.132103	0.420403	0.001384	0.714057
-7.572180	-1.954549	0.425408	0.001618	0.713965
-6.689778	-2.107559	0.430413	0.001453	0.713973
-6.873548	-2.080633	0.435418	0.001488	0.713961
-7.351857	-1.991019	0.440422	0.001577	0.713970
-7.062245	-2.079576	0.445427	0.001523	0.713897
-7.791416	-2.075902	0.450432	0.001659	0.713646
-7.849094	-2.061780	0.455437	0.001669	0.713653
-7.920418	-2.054452	0.460442	0.001683	0.713642
-7.605449	-2.106606	0.465446	0.001624	0.713650
-7.862215	-2.060821	0.470451	0.001672	0.713650
-8.305772	-2.064541	0.475456	0.001755	0.713486
-8.717213	-2.052262	0.480461	0.001831	0.713364
-8.405670	-2.112598	0.485466	0.001773	0.713354
-8.797242	-2.039891	0.490470	0.001846	0.713360
-8.869013	-2.027497	0.495475	0.001860	0.713359
-8.788216	-2.042797	0.500480	0.001845	0.713357
-8.895526	-2.108469	0.505485	0.001865	0.713189
-10.309592	-1.942309	0.510490	0.002128	0.713018
-9.776291	-2.034233	0.515494	0.002029	0.713024
-9.518329	-2.080118	0.520499	0.001981	0.713024
-10.050866	-1.988059	0.525504	0.002080	0.713018
-9.615607	-2.060946	0.530509	0.001999	0.713028
-9.787529	-2.034002	0.535514	0.002031	0.713020
-10.061131	-2.107878	0.540518	0.002082	0.712776
-10.551652	-2.053570	0.545523	0.002173	0.712710
-10.704425	-2.028075	0.550528	0.002202	0.712707
-10.660337	-2.034286	0.555533	0.002194	0.712710
-11.115223	-1.957824	0.560538	0.002278	0.712701
-10.503146	-2.062337	0.565542	0.002164	0.712710
-10.346930	-2.103816	0.570547	0.002135	0.712682
-11.677131	-2.017421	0.575552	0.002383	0.712382
-11.578407	-2.032114	0.580557	0.002365	0.712388
-11.651396	-2.023225	0.585562	0.002378	0.712380
-11.705170	-2.010471	0.590566	0.002388	0.712386
-11.619786	-2.025256	0.595571	0.002373	0.712387
-11.860008	-1.985119	0.600576	0.002417	0.712381
-11.537691	-2.039926	0.605581	0.002357	0.712387
-12.016197	-2.079133	0.610586	0.002447	0.712138
-12.688886	-1.984026	0.615590	0.002572	0.712089
-12.421300	-2.031591	0.620595	0.002522	0.712089
-12.675351	-1.987577	0.625600	0.002569	0.712087
-12.647358	-1.989238	0.630605	0.002564	0.712093
-12.640798	-1.994913	0.635610	0.002563	0.712084
-12.469313	-2.022181	0.640614	0.002531	0.712091
-12.713385	-2.075892	0.645619	0.002577	0.711897
-13.674937	-1.975265	0.650624	0.002756	0.711756
-13.373616	-2.024065	0.655629	0.002700	0.711765
-13.774178	-1.956566	0.660634	0.002774	0.711758
-13.619371	-1.981060	0.665638	0.002745	0.711764
-13.206222	-2.055190	0.670643	0.002669	0.711763
-13.484466	-2.009761	0.675648	0.002720	0.711754
-13.304596	-2.099984	0.680653	0.002687	0.711638
-14.398252	-1.999892	0.685658	0.002891	0.711449
-14.366698	-2.002816	0.690662	0.002885	0.711454
-14.641089	-1.954118	0.695667	0.002936	0.711454
-14.615680	-1.960604	0.700672	0.002931	0.711450
-14.059004	-2.056085	0.705677	0.002828	0.711457
-14.534593	-1.976153	0.710682	0.002916	0.711448
-14.296276	-2.045307	0.715686	0.002872	0.711394
-14.831716	-2.077427	0.720691	0.002972	0.711140
-15.296256	-1.998404	0.725696	0.003058	0.711132
-15.183886	-2.012836	0.730701	0.003037	0.711143
-15.171003	-2.019241	0.735706	0.003035	0.711135
-15.385486	-1.977854	0.740710	0.003075	0.711141
-15.329423	-1.988511	0.745715	0.003064	0.711140
-15.265872	-2.023069	0.750720	0.003053	0.711093
-15.701717	-2.054777	0.755725	0.003134	0.710875
-16.021667	-2.001555	0.760730	0.003193	0.710867
-15.936717	-2.015053	0.765734	0.003178	0.710871
-15.496091	-2.093223	0.770739	0.003096	0.710871
-15.910993	-2.021439	0.775744	0.003173	0.710867
-15.841110	-2.029554	0.780749	0.003160	0.710875
-15.890617	-2.150357	0.785754	0.003169	0.710617
-17.062170	-1.982969	0.790758	0.003387	0.710534
-17.166720	-1.963323	0.795763	0.003407	0.710536
-16.836753	-2.023729	0.800768	0.003346	0.710533
-16.708166	-2.041917	0.805773	0.003322	0.710542
-17.124153	-1.972555	0.810778	0.003399	0.710532
-16.900104	-2.011076	0.815782	0.003357	0.710535
-17.011597	-2.112954	0.820787	0.003378	0.710292
-18.067498	-1.962128	0.825792	0.003575	0.710217
-17.538300	-2.053352	0.830797	0.003476	0.710223
-17.434026	-2.075100	0.835802	0.003457	0.710217
-17.808992	-2.006912	0.840806	0.003527	0.710219
-17.927381	-1.986363	0.845811	0.003549	0.710218
-17.911695	-1.992831	0.850816	0.003546	0.710211
-18.043379	-2.102609	0.855821	0.003571	0.709944
-19.146503	-1.934052	0.860826	0.003776	0.709888
-18.847263	-1.983361	0.865830	0.003720	0.709896
-18.502048	-2.044690	0.870835	0.003656	0.709897
-19.066822	-1.946305	0.875840	0.003761	0.709892
-18.943967	-1.964219	0.880845	0.003739	0.709900
-18.745452	-2.004440	0.885850	0.003702	0.709890
-18.805889	-2.046137	0.890854	0.003713	0.709785
-19.575369	-2.002285	0.895859	0.003856	0.709598
-19.254620	-2.063040	0.900864	0.003797	0.709591
-19.280305	-2.054952	0.905869	0.003801	0.709598
-19.750718	-1.973771	0.910874	0.003889	0.709593
-19.556370	-2.007082	0.915878	0.003853	0.709595
-19.302543	-2.051306	0.920883	0.003806	0.709597
-19.825179	-2.071081	0.925888	0.003903	0.709371
-20.628446	-1.980194	0.930893	0.004053	0.709267
-20.300164	-2.042798	0.935898	0.003992	0.709258
-20.173889	-2.063042	0.940902	0.003968	0.709263
-20.525728	-1.999480	0.945907	0.004034	0.709265
-20.478938	-2.011604	0.950912	0.004025	0.709257
-20.143814	-2.067158	0.955917	0.003963	0.709265
-20.900069	-2.043134	0.960922	0.004103	0.709043
-21.517278	-1.976957	0.965926	0.004218	0.708956
-21.003047	-2.068647	0.970931	0.004123	0.708955
-21.266438	-2.023655	0.975936	0.004172	0.708951
-21.268888	-2.017723	0.980941	0.004172	0.708962
-21.091428	-2.054693	0.985946	0.004139	0.708952
-21.205046	-2.032496	0.990950	0.004160	0.708955
-21.938792	-2.030551	0.995955	0.004297	0.708697
-22.754574	-1.918593	1.000960	0.004449	0.708630
-21.994385	-2.047964	1.005965	0.004308	0.708643
-22.293296	-1.998978	1.010970	0.004363	0.708634
-22.573168	-1.946877	1.015974	0.004415	0.708638
-22.303832	-1.994492	1.020979	0.004365	0.708639
-22.383262	-1.982324	1.025984	0.004380	0.708635
-22.435911	-1.988607	1.030989	0.004390	0.708603
-22.864097	-2.039728	1.035994	0.004470	0.708348
-22.771335	-2.054627	1.040998	0.004452	0.708351
-23.483628	-1.927324	1.046003	0.004585	0.708352
-23.190047	-1.983079	1.051008	0.004530	0.708345
-22.901450	-2.030467	1.056013	0.004477	0.708353
-23.465032	-1.933914	1.061018	0.004582	0.708345
-23.428834	-1.938926	1.066022	0.004575	0.708348
-23.098437	-2.150396	1.071027	0.004514	0.708042
-24.046238	-2.000113	1.076032	0.004690	0.708005
-24.258505	-1.957570	1.081037	0.004730	0.708014
-24.002037	-2.005775	1.086042	0.004682	0.708009
-24.055081	-1.996712	1.091046	0.004692	0.708008
-24.028950	-1.998918	1.096051	0.004687	0.708013
-24.284457	-1.959102	1.101056	0.004735	0.708001
-24.408215	-2.074835	1.106061	0.004758	0.707725
-24.802905	-2.019586	1.111066	0.004831	0.707695
-24.983499	-1.986036	1.116070	0.004865	0.707697
-24.764478	-2.023442	1.121075	0.004824	0.707700
-24.910532	-2.002275	1.126080	0.004851	0.707691
-24.852360	-2.007158	1.131085	0.004841	0.707701
-24.927486	-1.999878	1.136090	0.004855	0.707689
-25.392809	-2.074154	1.141094	0.004941	0.707374
-25.858058	-1.990177	1.146099	0.005028	0.707376
-26.509343	-1.877357	1.151104	0.005149	0.707369
-25.716277	-2.014673	1.156109	0.005002	0.707377
-25.965409	-1.973652	1.161114	0.005048	0.707370
-26.418144	-1.891556	1.166118	0.005132	0.707373
-25.877777	-1.985191	1.171123	0.005032	0.707378
-25.774200	-2.059466	1.176128	0.005013	0.707266
-27.050203	-1.923712	1.181133	0.005250	0.707082
-26.556532	-2.015092	1.186138	0.005158	0.707075
-26.698814	-1.987943	1.191142	0.005185	0.707079
-26.695901	-1.986403	1.196147	0.005184	0.707083
-26.777968	-1.976014	1.201152	0.005200	0.707074
-26.506478	-2.019821	1.206157	0.005149	0.707083
-26.763070	-2.035780	1.211162	0.005197	0.706959
-27.917478	-1.935177	1.216166	0.005412	0.706748
-27.593152	-1.991203	1.221171	0.005352	0.706752
-27.727325	-1.970979	1.226176	0.005377	0.706744
-27.479874	-2.009455	1.231181	0.005331	0.706755
-27.810709	-1.953476	1.236186	0.005392	0.706749
-27.951612	-1.928400	1.241190	0.005419	0.706749
-27.593869	-2.002818	1.246195	0.005352	0.706728
-28.549499	-1.979054	1.251200	0.005530	0.706433
-28.499868	-1.981221	1.256205	0.005521	0.706446
-28.753865	-1.939753	1.261210	0.005568	0.706439
-28.685180	-1.951687	1.266214	0.005555	0.706439
-28.375602	-2.004503	1.271219	0.005498	0.706444
-28.665206	-1.956454	1.276224	0.005552	0.706437
-28.619930	-1.958661	1.281229	0.005543	0.706448
-28.892598	-2.023341	1.286234	0.005594	0.706221
-29.675704	-1.931037	1.291238	0.005740	0.706125
-28.929084	-2.061918	1.296243	0.005601	0.706130
-29.600259	-1.946624	1.301248	0.005726	0.706121
-29.438793	-1.969546	1.306253	0.005696	0.706133
-29.061137	-2.040828	1.311258	0.005626	0.706125
-29.315452	-1.995418	1.316262	0.005673	0.706125
-29.896167	-2.019644	1.321267	0.005781	0.705868
-30.355386	-1.945079	1.326272	0.005867	0.705853
-30.091719	-1.988086	1.331277	0.005818	0.705861
-30.185621	-1.972900	1.336282	0.005835	0.705858
-30.138352	-1.981522	1.341286	0.005827	0.705857
-29.884765	-2.024478	1.346291	0.005779	0.705862
-30.299121	-2.000712	1.351296	0.005857	0.705761
-31.019746	-1.989414	1.356301	0.005991	0.705525
-30.656566	-2.058193	1.361306	0.005923	0.705517
-31.398373	-1.925721	1.366310	0.006061	0.705517
-31.109466	-1.973851	1.371315	0.006008	0.705524
-30.930955	-2.007769	1.376320	0.005974	0.705520
-30.862398	-2.017005	1.381325	0.005962	0.705526
-31.484357	-1.981916	1.386330	0.006077	0.705373
-32.146144	-1.946106	1.391334	0.006201	0.705208
-31.377492	-2.079608	1.396339	0.006058	0.705215
-32.036714	-1.966120	1.401344	0.006180	0.705207
-32.145910	-1.943243	1.406349	0.006201	0.705213
-31.882315	-1.993726	1.411354	0.006152	0.705206
-31.902613	-1.988674	1.416358	0.006156	0.705209
-31.983310	-2.065272	1.421363	0.006171	0.705026
-32.955437	-1.962737	1.426368	0.006352	0.704883
-32.485508	-2.042950	1.431373	0.006264	0.704890
-32.959499	-1.960930	1.436378	0.006353	0.704885
-33.057999	-1.941976	1.441382	0.006371	0.704888
-32.563759	-2.028500	1.446387	0.006279	0.704891
-32.991306	-1.957085	1.451392	0.006359	0.704881
-33.002130	-2.049466	1.456397	0.006361	0.704691
-33.694031	-1.977251	1.461402	0.006490	0.704588
-33.541331	-2.005095	1.466406	0.006461	0.704587
-33.808163	-1.954775	1.471411	0.006511	0.704592
-33.858334	-1.951526	1.476416	0.006520	0.704581
-33.314673	-2.043958	1.481421	0.006419	0.704590
-33.876210	-1.944933	1.486426	0.006524	0.704587
-34.179955	-2.007084	1.491430	0.006580	0.704353
-34.385359	-2.015766	1.496435	0.006619	0.704262
-34.765943	-1.952523	1.501440	0.006689	0.704252
-34.790630	-1.944561	1.506445	0.006694	0.704259
-34.430561	-2.010421	1.511450	0.006627	0.704256
-34.471029	-2.004369	1.516454	0.006635	0.704253
-34.722062	-1.956208	1.521459	0.006681	0.704260
-34.931892	-2.012132	1.526464	0.006721	0.704072
-35.616719	-1.948555	1.531469	0.006848	0.703954
-35.531625	-1.967404	1.536474	0.006832	0.703946
-35.793267	-1.920835	1.541478	0.006881	0.703946
-35.363317	-1.994550	1.546483	0.006801	0.703952
-35.396720	-1.995136	1.551488	0.006807	0.703939
-35.354626	-1.996799	1.556493	0.006799	0.703950
-35.313700	-2.075488	1.561498	0.006792	0.703806
-36.315210	-1.986524	1.566502	0.006978	0.703626
-36.153748	-2.011019	1.571507	0.006948	0.703634
-36.566867	-1.941504	1.576512	0.007025	0.703626
-36.128299	-2.016720	1.581517	0.006944	0.703632
-36.247607	-1.996687	1.586522	0.006966	0.703629
-36.647125	-1.925303	1.591526	0.007040	0.703629
-36.242667	-2.081921	1.596531	0.006965	0.703459
-37.278170	-1.959822	1.601536	0.007158	0.703332
-37.237883	-1.963759	1.606541	0.007150	0.703339
-37.220189	-1.969118	1.611546	0.007147	0.703334
-37.061500	-1.995983	1.616550	0.007118	0.703337
-37.048848	-1.996152	1.621555	0.007115	0.703341
-37.352635	-1.945353	1.626560	0.007172	0.703334
-37.334881	-2.073610	1.631565	0.007169	0.703082
-38.078332	-1.980667	1.636570	0.007307	0.703002
-38.201906	-1.959949	1.641574	0.007330	0.702999
-37.850045	-2.019943	1.646579	0.007265	0.703004
-38.179298	-1.963944	1.651584	0.007326	0.702999
-38.326839	-1.934354	1.656589	0.007354	0.703005
-38.217280	-1.956054	1.661594	0.007333	0.703001
-38.374299	-2.041999	1.666598	0.007363	0.702771
-38.930880	-1.981930	1.671603	0.007466	0.702692
-39.148971	-1.947216	1.676608	0.007507	0.702683
-38.727608	-2.018601	1.681613	0.007429	0.702691
-38.756093	-2.014643	1.686618	0.007434	0.702688
-39.113272	-1.952542	1.691622	0.007500	0.702685
-38.872010	-1.992896	1.696627	0.007455	0.702690
-39.299038	-2.051379	1.701632	0.007535	0.702418
-40.000212	-1.951529	1.706637	0.007666	0.702367
-39.790874	-1.990749	1.711642	0.007627	0.702363
-39.352472	-2.070850	1.716646	0.007545	0.702359
-39.529185	-2.035327	1.721651	0.007578	0.702367
-39.870386	-1.977270	1.726656	0.007642	0.702362
-39.797098	-1.996979	1.731661	0.007628	0.702348
-40.375953	-2.031561	1.736666	0.007736	0.702069
-40.823455	-1.953389	1.741670	0.007819	0.702066
-40.788982	-1.956874	1.746675	0.007813	0.702071
-40.549726	-2.003435	1.751680	0.007768	0.702063
-40.764013	-1.960865	1.756685	0.007808	0.702072
-40.937774	-1.931349	1.761690	0.007841	0.702069
-40.697534	-1.975693	1.766694	0.007796	0.702066
-40.858092	-2.083569	1.771699	0.007826	0.701790
-41.767091	-1.949216	1.776704	0.007995	0.701733
-41.682844	-1.959225	1.781709	0.007980	0.701744
-41.321782	-2.026232	1.786714	0.007912	0.701738
-41.973488	-1.912261	1.791718	0.008034	0.701734
-41.627576	-1.968891	1.796723	0.007969	0.701744
-41.254968	-2.040502	1.801728	0.007900	0.701733
-42.133292	-2.015307	1.806733	0.008064	0.701467
-42.730629	-1.925718	1.811738	0.008175	0.701433
-42.614581	-1.946875	1.816742	0.008153	0.701432
-42.080394	-2.037467	1.821747	0.008054	0.701441
-42.808002	-1.913466	1.826752	0.008189	0.701429
-42.433625	-1.975715	1.831757	0.008120	0.701438
-42.194226	-2.020140	1.836762	0.008075	0.701435
-42.960953	-2.010583	1.841766	0.008218	0.701177
-43.643613	-1.913900	1.846771	0.008345	0.701126
-43.312726	-1.979919	1.851776	0.008284	0.701112
-42.931253	-2.043321	1.856781	0.008213	0.701121
-43.508587	-1.941720	1.861786	0.008320	0.701119
-43.481944	-1.948668	1.866790	0.008315	0.701114
-42.848473	-2.055735	1.871795	0.008197	0.701126
-43.665599	-2.021836	1.876800	0.008349	0.700899
-43.832323	-2.003856	1.881805	0.008381	0.700876
-43.829211	-2.005606	1.886810	0.008380	0.700873
-44.185550	-1.945067	1.891814	0.008446	0.700867
-44.050235	-1.963767	1.896819	0.008421	0.700878
-43.831713	-2.007282	1.901824	0.008381	0.700869
-43.889427	-2.083999	1.906829	0.008391	0.700692
-45.370143	-1.898730	1.911834	0.008667	0.700532
-45.072666	-1.953320	1.916838	0.008612	0.700529
-44.341414	-2.079644	1.921843	0.008476	0.700537
-44.970254	-1.972625	1.926848	0.008593	0.700527
-44.837870	-1.992076	1.931853	0.008568	0.700535
-44.610735	-2.033737	1.936858	0.008526	0.700533
-45.508075	-2.016487	1.941862	0.008693	0.700243
-45.640066	-2.003879	1.946867	0.008718	0.700221
-45.807902	-1.980607	1.951872	0.008749	0.700207
-45.605979	-2.013924	1.956877	0.008711	0.700213
-45.698040	-1.996738	1.961882	0.008729	0.700214
-45.901764	-1.961332	1.966886	0.008767	0.700212
-45.372860	-2.084439	1.971891	0.008668	0.700154
-46.700071	-1.978557	1.976896	0.008915	0.699888
-46.590828	-1.996040	1.981901	0.008895	0.699892
-46.398858	-2.031777	1.986906	0.008859	0.699889
-46.689866	-1.980188	1.991910	0.008913	0.699889
-46.618356	-1.989826	1.996915	0.008900	0.699895
-46.379256	-2.056816	2.001920	0.008856	0.699845
-47.466218	-1.988071	2.011917	0.009058	0.699591
-47.439055	-1.991647	2.021914	0.009053	0.699594
-47.386943	-1.999980	2.031910	0.009044	0.699596
-47.334737	-2.010679	2.041907	0.009034	0.699593
-47.535635	-1.974583	2.051904	0.009071	0.699593
-47.422790	-1.993863	2.061901	0.009051	0.699594
-47.262176	-2.021123	2.071898	0.009021	0.699597
-47.251203	-2.023236	2.081894	0.009019	0.699597
-47.383823	-1.999664	2.091891	0.009043	0.699596
-47.414118	-1.994764	2.101888	0.009049	0.699595
-47.266792	-1.929482	2.111885	0.009022	0.699781
-46.538961	-2.004868	2.121882	0.008886	0.699891
-46.709963	-1.974027	2.131878	0.008918	0.699892
-46.648660	-1.985193	2.141875	0.008907	0.699891
-46.585638	-1.998129	2.151872	0.008895	0.699887
-46.598346	-1.994787	2.161869	0.008898	0.699890
-45.924783	-1.976307	2.171866	0.008772	0.700171
-45.708923	-1.990760	2.181862	0.008732	0.700219
-45.411088	-2.044493	2.191859	0.008677	0.700218
-45.612867	-2.009821	2.201856	0.008715	0.700215
-45.747937	-1.960496	2.211853	0.008740	0.700266
-44.693406	-2.017507	2.221850	0.008544	0.700532
-44.868052	-1.985632	2.231846	0.008576	0.700533
-44.741557	-2.007730	2.241843	0.008553	0.700534
-44.667240	-2.015626	2.251840	0.008539	0.700544
-44.149794	-1.947142	2.261837	0.008443	0.700870
-43.818505	-2.005257	2.271834	0.008381	0.700872
-43.917511	-1.988414	2.281830	0.008400	0.700870
-43.726533	-1.996822	2.291827	0.008364	0.700922
-43.183980	-1.996586	2.301824	0.008263	0.701118
-43.166241	-2.000176	2.311821	0.008260	0.701117
-43.056741	-2.019551	2.321818	0.008240	0.701117
-42.633034	-1.996086	2.331814	0.008161	0.701318
-42.242483	-2.008526	2.341811	0.008088	0.701433
-42.556111	-1.954147	2.351808	0.008147	0.701430
-42.244193	-1.971474	2.361805	0.008089	0.701507
-41.288752	-2.026854	2.371802	0.007911	0.701740
-41.644194	-1.963206	2.381798	0.007977	0.701740
-41.402910	-2.005499	2.391795	0.007932	0.701742
-40.987689	-1.944418	2.401792	0.007855	0.702015
-40.517194	-2.000804	2.411789	0.007767	0.702070
-40.497465	-2.003243	2.421786	0.007764	0.702072
-40.457228	-1.959644	2.431782	0.007756	0.702175
-39.603103	-2.016320	2.441779	0.007597	0.702368
-39.613875	-2.015368	2.451776	0.007600	0.702366
-39.616943	-2.013703	2.461773	0.007600	0.702368
-39.040075	-1.990016	2.471770	0.007493	0.702624
-38.912341	-1.978220	2.481766	0.007469	0.702693
-38.740664	-2.008910	2.491763	0.007437	0.702693
-38.862555	-1.933648	2.501760	0.007460	0.702801
-37.759351	-2.031041	2.511757	0.007255	0.703002
-37.844119	-2.016007	2.521754	0.007271	0.703001
-37.785212	-2.024578	2.531750	0.007260	0.703005
-37.281096	-1.986634	2.541747	0.007166	0.703263
-37.301347	-1.946483	2.551744	0.007170	0.703337
-37.066197	-1.988025	2.561741	0.007126	0.703337
-36.833670	-1.981672	2.571738	0.007083	0.703434
-36.256161	-1.985817	2.581734	0.006975	0.703633
-36.102008	-2.013342	2.591731	0.006947	0.703633
-36.292971	-1.980034	2.601728	0.006982	0.703631
-35.318599	-2.016316	2.611725	0.006801	0.703908
-35.503328	-1.962576	2.621722	0.006835	0.703950
-35.184818	-2.018629	2.631718	0.006776	0.703951
-35.079392	-1.984068	2.641715	0.006757	0.704059
-34.376198	-2.011997	2.651712	0.006626	0.704255
-34.351315	-2.015544	2.661709	0.006621	0.704257
-34.362168	-2.011945	2.671706	0.006623	0.704260
-33.810117	-1.995214	2.681702	0.006521	0.704492
-33.616696	-1.981261	2.691699	0.006485	0.704589
-33.636422	-1.978717	2.701696	0.006488	0.704587
-33.176765	-2.026263	2.711693	0.006403	0.704656
-32.819619	-1.975296	2.721690	0.006337	0.704887
-32.511023	-2.028995	2.731686	0.006279	0.704890
-32.892515	-1.962888	2.741683	0.006350	0.704886
-32.029789	-1.982373	2.751680	0.006190	0.705156
-32.005929	-1.959611	2.761677	0.006185	0.705210
-31.864965	-1.985093	2.771674	0.006159	0.705209
-31.555249	-1.971706	2.781670	0.006102	0.705347
-31.041145	-1.976060	2.791667	0.006006	0.705523
-30.960729	-1.990748	2.801664	0.005991	0.705522
-30.872978	-2.006394	2.811661	0.005975	0.705522
-30.418721	-1.922699	2.821658	0.005890	0.705853
-29.766679	-2.034080	2.831654	0.005769	0.705863
-29.923023	-2.006407	2.841651	0.005798	0.705862
-29.830472	-1.985330	2.851648	0.005781	0.705937
-29.123111	-2.019584	2.861645	0.005649	0.706122
-29.184152	-2.006645	2.871642	0.005661	0.706126
-29.209995	-2.001847	2.881638	0.005666	0.706126
-28.871679	-1.920396	2.891635	0.005603	0.706411
-28.317817	-2.005284	2.901632	0.005500	0.706439
-28.432966	-1.985266	2.911629	0.005521	0.706437
-27.986214	-1.976143	2.921626	0.005438	0.706616
-27.576978	-1.982254	2.931622	0.005362	0.706750
-27.623330	-1.974812	2.941619	0.005371	0.706748
-27.273625	-2.010886	2.951616	0.005306	0.706800
-26.696902	-1.975679	2.961613	0.005198	0.707077
-26.393281	-2.030191	2.971610	0.005142	0.707076
-26.614916	-1.990260	2.981606	0.005183	0.707077
-26.295210	-1.954238	2.991603	0.005124	0.707264
-25.802980	-1.988472	3.001600	0.005032	0.707371
-26.185794	-1.919656	3.011597	0.005104	0.707372
-25.680341	-1.954369	3.021594	0.005010	0.707483
-24.831182	-1.997776	3.031590	0.004852	0.707699
-25.053445	-1.957267	3.041587	0.004893	0.707701
-25.048430	-1.955826	3.051584	0.004892	0.707706
-24.434478	-1.912173	3.061581	0.004778	0.708012
-24.052659	-1.979139	3.071578	0.004707	0.708014
-24.002211	-1.987588	3.081574	0.004698	0.708015
-23.628308	-1.955907	3.091571	0.004628	0.708212
-23.112964	-1.979048	3.101568	0.004532	0.708350
-23.210988	-1.960722	3.111565	0.004550	0.708351
-22.896915	-2.016547	3.121562	0.004492	0.708352
-22.583843	-1.936440	3.131558	0.004434	0.708624
-22.263630	-1.984307	3.141555	0.004374	0.708642
-22.046500	-2.025272	3.151552	0.004334	0.708637
-22.246723	-1.933126	3.161549	0.004371	0.708750
-21.296045	-1.999134	3.171546	0.004194	0.708957
-21.645490	-1.936467	3.181542	0.004259	0.708958
-21.363360	-1.986792	3.191539	0.004207	0.708957
-20.828081	-1.929137	3.201536	0.004107	0.709264
-20.737997	-1.944336	3.211533	0.004091	0.709265
-20.556781	-1.976128	3.221530	0.004057	0.709266
-20.320559	-1.907962	3.231526	0.004013	0.709487
-19.706021	-1.962399	3.241523	0.003899	0.709597
-19.764304	-1.953109	3.251520	0.003910	0.709594
-19.821214	-1.902800	3.261517	0.003920	0.709674
-18.835878	-1.968540	3.271514	0.003737	0.709894
-18.774458	-1.980349	3.281510	0.003726	0.709892
-18.709580	-1.992579	3.291507	0.003714	0.709891
-18.406674	-1.926887	3.301504	0.003657	0.710130
-18.210001	-1.919275	3.311501	0.003621	0.710215
-18.020291	-1.950388	3.321498	0.003586	0.710220
-17.916671	-1.906629	3.331494	0.003566	0.710344
-16.855269	-2.001810	3.341491	0.003369	0.710532
-17.121856	-1.955206	3.351488	0.003419	0.710530
-16.998662	-1.975677	3.361485	0.003396	0.710533
-16.451523	-1.951475	3.371482	0.003294	0.710775
-16.024253	-1.979158	3.381478	0.003214	0.710872
-16.094777	-1.967181	3.391475	0.003228	0.710871
-16.147293	-1.953246	3.401472	0.003237	0.710880
-15.538204	-1.932970	3.411469	0.003124	0.711137
-15.271807	-1.979505	3.421466	0.003075	0.711138
-15.351227	-1.965551	3.431462	0.003089	0.711138
-14.838536	-1.958917	3.441459	0.002994	0.711333
-14.742476	-1.916645	3.451456	0.002976	0.711452
-14.645701	-1.933345	3.461453	0.002958	0.711453
-14.338426	-1.944532	3.471450	0.002901	0.711539
-13.430651	-1.994126	3.481446	0.002732	0.711763
-13.618486	-1.961796	3.491443	0.002767	0.711760
-13.913788	-1.910277	3.501440	0.002822	0.711758
-12.905007	-1.949048	3.511437	0.002635	0.712039
-12.743596	-1.952245	3.521434	0.002605	0.712090
-12.773485	-1.945942	3.531430	0.002610	0.712091
-12.411736	-1.962752	3.541427	0.002543	0.712186
-11.783571	-1.976966	3.551424	0.002426	0.712381
-11.716363	-1.988396	3.561421	0.002414	0.712382
-11.890469	-1.957219	3.571418	0.002446	0.712382
-11.360379	-1.943097	3.581414	0.002348	0.712598
-11.048757	-1.943244	3.591411	0.002290	0.712708
-11.126380	-1.931615	3.601408	0.002304	0.712704
-10.791607	-1.950482	3.611405	0.002242	0.712785
-10.012977	-1.969502	3.621402	0.002097	0.713023
-9.852904	-1.999244	3.631398	0.002067	0.713020
-10.003686	-1.972814	3.641395	0.002095	0.713019
-9.818241	-1.897808	3.651392	0.002061	0.713234
-8.843197	-2.010014	3.661389	0.001880	0.713356
-8.937896	-1.992909	3.671386	0.001897	0.713356
-8.561238	-2.058529	3.681382	0.001827	0.713359
-8.236618	-2.008539	3.691379	0.001767	0.713574
-7.913699	-2.029915	3.701376	0.001707	0.713645
-7.776099	-2.054513	3.711373	0.001681	0.713645
-8.178217	-1.981104	3.721370	0.001756	0.713648
-7.125274	-2.037432	3.731366	0.001560	0.713909
-7.067864	-2.017739	3.741363	0.001550	0.713968
-7.136220	-2.005013	3.751360	0.001562	0.713969
-7.045147	-2.014479	3.761357	0.001545	0.713983
-6.483935	-1.967984	3.771354	0.001441	0.714274
-5.860712	-2.077093	3.781350	0.001325	0.714277
-6.088007	-2.036406	3.791347	0.001368	0.714277
-6.019271	-1.997741	3.801344	0.001355	0.714378
-5.004636	-2.064886	3.811341	0.001166	0.714604
-5.019509	-2.060312	3.821338	0.001169	0.714608
-5.121941	-2.041161	3.831334	0.001188	0.714609
-5.066608	-1.968705	3.841331	0.001178	0.714772
-4.349347	-2.030417	3.851328	0.001044	0.714903
-4.510590	-2.001144	3.861325	0.001074	0.714904
-4.388512	-2.006356	3.871322	0.001052	0.714937
-3.557980	-2.007983	3.881318	0.000897	0.715227
-3.469837	-2.022823	3.891315	0.000881	0.715229
-3.458107	-2.026374	3.901312	0.000879	0.715226
-3.019972	-2.025545	3.911309	0.000797	0.715382
-2.466670	-2.043794	3.921306	0.000694	0.715541
-2.142166	-2.101724	3.931302	0.000634	0.715541
-2.501639	-2.035404	3.941299	0.000701	0.715545
-1.868082	-2.039975	3.951296	0.000583	0.715760
-1.699396	-2.011116	3.961293	0.000552	0.715876
-1.534715	-2.040140	3.971290	0.000521	0.715877
-1.528416	-2.040202	3.981286	0.000520	0.715879
-1.265569	-1.961204	3.991283	0.000471	0.716128
-1.125421	-1.986883	4.001280	0.000445	0.716126
-1.024086	-2.004071	4.011277	0.000426	0.716128
-0.954437	-1.872260	4.021274	0.000413	0.716413
-0.990516	-1.849261	4.031270	0.000420	0.716446
-0.790603	-1.830090	4.041267	0.000383	0.716554
-0.612133	-1.761763	4.051264	0.000350	0.716752
-0.565930	-1.768536	4.061261	0.000341	0.716755
-0.508475	-1.612146	4.071258	0.000331	0.717085
-0.517354	-1.609976	4.081254	0.000332	0.717086
-0.302574	-1.505560	4.091251	0.000292	0.717368
-0.291713	-1.494654	4.101248	0.000290	0.717393
-0.238570	-1.349089	4.111245	0.000280	0.717699
-0.366972	-1.276046	4.121242	0.000304	0.717798
-0.304942	-1.177388	4.131238	0.000293	0.718015
-0.142341	-1.079516	4.141235	0.000263	0.718265
-0.291210	-0.971880	4.151232	0.000290	0.718425
-0.059811	-0.904162	4.161229	0.000247	0.718640
-0.105766	-0.757232	4.171226	0.000256	0.718914
0.139176	-0.699021	4.181222	0.000210	0.719115
0.105770	-0.579319	4.191219	0.000216	0.719339
0.053850	-0.438724	4.201216	0.000226	0.719598
-0.044377	-0.273218	4.211213	0.000244	0.719889
0.059647	-0.150892	4.221210	0.000225	0.720167
0.056861	-0.009370	4.231206	0.000225	0.720444
0.000000	0.155951	4.241203	0.000236	0.720750
0.274388	0.725169	4.246208	0.000185	0.721965
0.360276	1.981848	4.251213	0.000168	0.724460
0.480131	3.817490	4.256218	0.000144	0.728087
0.957802	6.147403	4.261222	0.000054	0.732777
1.131999	9.033516	4.266227	0.000020	0.738402
1.548032	12.363686	4.271232	-0.000060	0.744913
1.750503	16.177620	4.276237	-0.000100	0.752209
2.268732	20.343218	4.281242	-0.000199	0.760195
2.651436	24.935055	4.286246	-0.000273	0.768841
2.989881	29.900924	4.291251	-0.000340	0.778058
3.552556	35.176202	4.296256	-0.000448	0.787796
4.069332	40.776961	4.301261	-0.000548	0.797979
4.322362	46.726232	4.306266	-0.000599	0.808564
4.700701	52.936373	4.311270	-0.000673	0.819501
5.005277	59.426001	4.316275	-0.000734	0.830749
5.616366	66.089168	4.321280	-0.000852	0.842230
6.227790	72.969036	4.326285	-0.000970	0.853917
6.787807	80.076850	4.331290	-0.001079	0.865804
7.150294	87.400110	4.336294	-0.001151	0.877822
13.599252	93.856432	4.341299	-0.002356	0.890000
16.732963	101.175997	4.346304	-0.002945	0.902452
17.052473	109.130804	4.351309	-0.003009	0.914953
17.488395	117.168559	4.356314	-0.003096	0.927442
17.824834	125.330503	4.361318	-0.003164	0.939927
18.782637	133.480750	4.366323	-0.003347	0.952392
19.726751	141.728229	4.371328	-0.003528	0.964835
20.175937	150.123242	4.376333	-0.003617	0.977207
21.320652	158.484956	4.381338	-0.003836	0.989551
22.488566	166.885724	4.386342	-0.004059	1.001802
23.193130	175.397566	4.391347	-0.004196	1.013948
24.301621	183.884241	4.396352	-0.004407	1.026012
25.316805	192.424441	4.401357	-0.004602	1.037985
26.171274	201.029702	4.406362	-0.004767	1.049872
27.314828	209.601196	4.411366	-0.004985	1.061647
28.106996	218.269509	4.416371	-0.005138	1.073340
29.085094	226.892751	4.421376	-0.005326	1.084889
30.141644	235.520397	4.426381	-0.005528	1.096340
30.803134	244.218766	4.431386	-0.005657	1.107675
31.654813	252.888448	4.436390	-0.005821	1.118899
32.264855	261.588188	4.441395	-0.005941	1.129998
33.075622	270.258758	4.446400	-0.006097	1.140995
33.781109	278.952597	4.451405	-0.006234	1.151892
34.549948	287.602020	4.456410	-0.006383	1.162647
35.300291	296.240072	4.461414	-0.006528	1.173284
36.047108	304.848132	4.466419	-0.006673	1.183790
37.162562	313.411796	4.471424	-0.006886	1.194224
37.850257	322.014832	4.476429	-0.007020	1.204528
38.882800	330.573930	4.481434	-0.007217	1.214761
39.625166	339.158871	4.486438	-0.007361	1.224881
40.206152	347.777655	4.491443	-0.007475	1.234926
40.993342	356.313053	4.496448	-0.007627	1.244833
41.841977	364.827993	4.501453	-0.007791	1.254651
42.854047	373.311147	4.506458	-0.007985	1.264388
43.453714	381.870435	4.511462	-0.008102	1.274057
43.790067	390.417088	4.516467	-0.008170	1.283589
44.636529	398.902724	4.521472	-0.008333	1.293079
45.588311	407.339726	4.526477	-0.008516	1.302466
46.294540	415.902796	4.531482	-0.008653	1.311876
47.386895	424.332496	4.536486	-0.008862	1.321146
47.904391	432.780472	4.541491	-0.008963	1.330267
48.640138	441.192238	4.546496	-0.009106	1.339326
49.513220	449.560940	4.551501	-0.009274	1.348303
50.358619	457.954576	4.556506	-0.009437	1.357242
50.919212	466.357291	4.561510	-0.009546	1.366082
51.378585	474.782561	4.566515	-0.009637	1.374870
52.093178	483.151981	4.571520	-0.009776	1.383589
52.903500	491.513755	4.576525	-0.009932	1.392261
53.761704	499.841680	4.581530	-0.010097	1.400853
54.171918	508.233526	4.586534	-0.010179	1.409382
54.698072	516.593667	4.591539	-0.010283	1.417847
55.709346	524.864594	4.596544	-0.010476	1.426253
56.339580	533.208852	4.601549	-0.010599	1.434619
57.073922	541.518689	4.606554	-0.010741	1.442920
57.460558	549.886089	4.611558	-0.010819	1.451173
58.306805	558.160731	4.616563	-0.010981	1.459362
59.311759	566.426615	4.621568	-0.011174	1.467522
59.531531	574.849170	4.626573	-0.011220	1.475664
60.093514	583.128325	4.631578	-0.011330	1.483677
60.631195	591.421190	4.636582	-0.011436	1.491656
61.320849	599.668628	4.641587	-0.011569	1.499573
62.071627	607.916577	4.646592	-0.011715	1.507458
62.443491	616.227904	4.651597	-0.011789	1.515304
62.982762	624.492312	4.656602	-0.011895	1.523090
63.592241	632.746330	4.661606	-0.012014	1.530838
64.199651	640.989228	4.666611	-0.012132	1.538535
64.805104	649.247612	4.671616	-0.012250	1.546208
65.375145	657.516737	4.676621	-0.012362	1.553848
65.692167	665.785456	4.681626	-0.012426	1.561412
66.394509	673.991826	4.686630	-0.012562	1.568940
67.224616	682.180875	4.691635	-0.012722	1.576435
67.731984	690.430343	4.696640	-0.012822	1.583901
68.007386	698.700419	4.701645	-0.012879	1.591317
68.433026	706.939307	4.706650	-0.012963	1.598693
68.848396	715.163026	4.711654	-0.013046	1.606019
69.320054	723.386992	4.716659	-0.013139	1.613320
70.021473	731.578420	4.721664	-0.013275	1.620592
70.493551	739.794462	4.726669	-0.013368	1.627821
70.947988	748.076743	4.731674	-0.013458	1.635072
71.436830	756.254173	4.736678	-0.013554	1.642206
72.204451	764.403140	4.741683	-0.013703	1.649322
72.884607	772.593346	4.746688	-0.013835	1.656431
73.675428	780.719407	4.751693	-0.013987	1.663470
74.075639	788.944269	4.756698	-0.014067	1.670510
74.668705	797.144135	4.761702	-0.014183	1.677524
74.834722	805.348571	4.766707	-0.014219	1.684457
75.544102	813.514703	4.771712	-0.014356	1.691401
75.783690	821.738274	4.776717	-0.014406	1.698302
76.140288	829.919978	4.781722	-0.014478	1.705155
76.888394	838.082765	4.786726	-0.014622	1.712017
77.467471	846.239383	4.791731	-0.014736	1.718824
77.759985	854.425490	4.796736	-0.014795	1.725591
78.453440	862.571969	4.801741	-0.014930	1.732351
78.942215	870.750115	4.806746	-0.015026	1.739083
79.387352	878.910531	4.811750	-0.015114	1.745770
79.669894	887.116743	4.816755	-0.015172	1.752448
79.961555	895.299615	4.821760	-0.015232	1.759082
80.568393	903.400881	4.826765	-0.015350	1.765665
81.033297	911.583657	4.831770	-0.015442	1.772272
81.407448	919.759791	4.836774	-0.015517	1.778836
81.579295	927.934175	4.841779	-0.015554	1.785351
82.051183	936.129404	4.846784	-0.015647	1.791895
82.505896	944.269492	4.851789	-0.015737	1.798369
83.241468	952.349540	4.856794	-0.015879	1.804807
83.773576	960.491422	4.861798	-0.015984	1.811246
84.045714	968.661055	4.866803	-0.016040	1.817652
84.736100	976.769160	4.871808	-0.016173	1.824038
85.062920	984.936909	4.876813	-0.016240	1.830404
85.180506	993.127526	4.881818	-0.016267	1.836740
85.780542	1001.218606	4.886822	-0.016384	1.843036
86.601156	1009.288599	4.891827	-0.016542	1.849319
87.119453	1017.456262	4.896832	-0.016643	1.855620
87.461645	1025.592071	4.901837	-0.016712	1.861855
88.478363	1033.659639	4.906842	-0.016907	1.868096
89.013010	1041.834282	4.911846	-0.017012	1.874340
89.468067	1049.946782	4.916851	-0.017102	1.880508
90.094350	1058.068824	4.921856	-0.017224	1.886682
90.228933	1066.260858	4.926861	-0.017254	1.892833
90.701410	1074.389013	4.931866	-0.017347	1.898954
91.143197	1082.509620	4.936870	-0.017435	1.905046
91.602982	1090.641053	4.941875	-0.017526	1.911129
92.107111	1098.779429	4.946880	-0.017625	1.917202
92.537150	1106.884200	4.951885	-0.017710	1.923223
93.072123	1114.997240	4.956890	-0.017815	1.929242
93.551419	1123.134676	4.961894	-0.017909	1.935255
93.623243	1131.285915	4.966899	-0.017928	1.941214
94.290415	1139.379727	4.971904	-0.018058	1.947178
94.572213	1147.558921	4.976909	-0.018115	1.953144
94.945491	1155.671666	4.981914	-0.018190	1.959053
95.333198	1163.764168	4.986918	-0.018268	1.964932
95.876641	1171.847112	4.991923	-0.018374	1.970802
96.162081	1179.994013	4.996928	-0.018432	1.976673
96.749661	1188.058475	5.001933	-0.018547	1.982500
97.356219	1196.155538	5.006938	-0.018665	1.988336
97.845565	1204.282457	5.011942	-0.018762	1.994162
98.062468	1212.394806	5.016947	-0.018807	1.999933
98.377082	1220.516744	5.021952	-0.018871	2.005704
98.952888	1228.603045	5.026957	-0.018983	2.011460
99.536794	1236.680650	5.031962	-0.019097	2.017194
100.209559	1244.759466	5.036966	-0.019228	2.022922
100.659850	1252.858521	5.041971	-0.019317	2.028625
101.000490	1261.042911	5.046976	-0.019386	2.034360
101.380563	1269.119525	5.051981	-0.019462	2.040008
101.811322	1277.194699	5.056986	-0.019547	2.045645
102.188405	1285.330031	5.061990	-0.019623	2.051302
102.464089	1293.446256	5.066995	-0.019679	2.056920
102.875621	1301.535681	5.072000	-0.019761	2.062517
103.187327	1309.640787	5.077005	-0.019824	2.068101
103.635793	1317.752230	5.082010	-0.019913	2.073687
104.283245	1325.806684	5.087014	-0.020039	2.079239
104.918737	1333.857557	5.092019	-0.020162	2.084772
105.181790	1341.995517	5.097024	-0.020217	2.090313
105.410579	1350.121181	5.102029	-0.020264	2.095827
105.910247	1358.197657	5.107034	-0.020363	2.101320
106.537078	1366.264021	5.112038	-0.020485	2.106804
106.665283	1374.444700	5.117043	-0.020514	2.112303
107.039114	1382.556917	5.122048	-0.020589	2.117764
107.390027	1390.614958	5.127053	-0.020659	2.123174
107.684239	1398.703403	5.132058	-0.020719	2.128584
107.778155	1406.839568	5.137062	-0.020742	2.133993
108.150453	1414.899378	5.142067	-0.020817	2.139364
108.527427	1422.970551	5.147072	-0.020892	2.144730
108.715731	1431.079985	5.152077	-0.020932	2.150089
109.127143	1439.166029	5.157082	-0.021014	2.155441
109.512890	1447.238243	5.162086	-0.021091	2.160768
109.884762	1455.296562	5.167091	-0.021166	2.166071
110.269002	1463.383705	5.172096	-0.021242	2.171382
110.742294	1471.462433	5.177101	-0.021336	2.176682
111.111590	1479.543471	5.182106	-0.021410	2.181960
111.461159	1487.628333	5.187110	-0.021480	2.187227
111.926166	1495.720002	5.192115	-0.021572	2.192496
112.365786	1503.804519	5.197120	-0.021659	2.197745
112.431754	1511.896286	5.202125	-0.021676	2.202952
112.863225	1519.962318	5.207130	-0.021762	2.208164
113.168639	1528.074518	5.212134	-0.021824	2.213381
113.371454	1536.149262	5.217139	-0.021867	2.218553
113.596692	1544.235934	5.222144	-0.021914	2.223723
113.943870	1552.302121	5.227149	-0.021984	2.228878
114.442674	1560.378596	5.232154	-0.022082	2.234041
114.872621	1568.445939	5.237158	-0.022168	2.239180
114.956997	1576.528850	5.242163	-0.022188	2.244287
115.618495	1584.580337	5.247168	-0.022317	2.249413
115.887959	1592.677373	5.252173	-0.022372	2.254522
116.479483	1600.713545	5.257178	-0.022488	2.259609
116.934358	1608.799473	5.262182	-0.022578	2.264703
116.996338	1616.917062	5.267187	-0.022594	2.269772
117.700826	1625.034485	5.272192	-0.022731	2.274884
118.012015	1633.072277	5.277197	-0.022794	2.279902
118.321072	1641.120481	5.282202	-0.022857	2.284915
118.595606	1649.203984	5.287206	-0.022913	2.289936
118.814448	1657.286243	5.292211	-0.022959	2.294940
119.148245	1665.361624	5.297216	-0.023026	2.299939
119.640830	1673.392317	5.302221	-0.023123	2.304913
120.059984	1681.467090	5.307226	-0.023207	2.309897
120.749738	1689.535098	5.312230	-0.023340	2.314888
121.039766	1697.585737	5.317235	-0.023399	2.319825
121.051120	1705.704591	5.322240	-0.023407	2.324769
121.534320	1713.766946	5.327245	-0.023502	2.329708
122.185575	1721.816412	5.332250	-0.023628	2.334642
122.827191	1729.865301	5.337254	-0.023753	2.339565
123.031175	1737.925994	5.342259	-0.023796	2.344448
123.500512	1746.019311	5.347264	-0.023889	2.349362
123.926456	1754.111602	5.352269	-0.023973	2.354262
124.298207	1762.159090	5.357274	-0.024048	2.359120
125.012383	1770.177244	5.362278	-0.024186	2.363979
125.246906	1778.255013	5.367283	-0.024235	2.368824
125.533738	1786.358178	5.372288	-0.024294	2.373678
125.855752	1794.424566	5.377293	-0.024359	2.378504
126.251657	1802.472391	5.382298	-0.024438	2.383314
126.404273	1810.579609	5.387302	-0.024471	2.388131
126.837683	1818.630890	5.392307	-0.024557	2.392927
127.539195	1826.666537	5.397312	-0.024693	2.397725
127.783386	1834.729315	5.402317	-0.024744	2.402494
127.865827	1842.811475	5.407322	-0.024764	2.407252
128.382003	1850.890923	5.412326	-0.024866	2.412032
128.907924	1858.936891	5.417331	-0.024969	2.416784
129.357949	1866.986648	5.422336	-0.025058	2.421523
129.758504	1875.045896	5.427341	-0.025138	2.426255
130.272059	1883.133062	5.432346	-0.025238	2.431002
130.780221	1891.241664	5.437350	-0.025338	2.435751
130.881483	1899.290686	5.442355	-0.025362	2.440426
131.212619	1907.329299	5.447360	-0.025429	2.445103
131.492257	1915.388127	5.452365	-0.025487	2.449779
131.678601	1923.477489	5.457370	-0.025526	2.454457
132.099460	1931.521831	5.462374	-0.025610	2.459117
132.362766	1939.549806	5.467379	-0.025664	2.463748
132.512740	1947.667279	5.472384	-0.025697	2.468412
132.714313	1955.750609	5.477389	-0.025740	2.473052
133.067679	1963.781619	5.482394	-0.025811	2.477664
133.264843	1971.829763	5.487398	-0.025853	2.482266
133.449844	1979.880001	5.492403	-0.025893	2.486860
133.806625	1987.956833	5.497408	-0.025964	2.491473
134.177747	1996.004565	5.502413	-0.026039	2.496062
134.275052	2004.068757	5.507418	-0.026062	2.500631
134.604859	2012.124142	5.512422	-0.026129	2.505204
134.961790	2020.162145	5.517427	-0.026200	2.509762
135.406399	2028.273412	5.522432	-0.026288	2.514358
135.571153	2036.307224	5.527437	-0.026324	2.518882
135.904953	2044.325836	5.532442	-0.026392	2.523401
136.345549	2052.382221	5.537446	-0.026479	2.527942
136.589767	2060.437361	5.542451	-0.026530	2.532459
137.131732	2068.476609	5.547456	-0.026636	2.536980
137.368655	2076.523943	5.552461	-0.026685	2.541476
137.965316	2084.523605	5.557466	-0.026801	2.545963
138.306023	2092.627173	5.562470	-0.026870	2.550482
138.341553	2100.740018	5.567475	-0.026882	2.554976
138.687516	2108.778961	5.572480	-0.026951	2.559444
138.984499	2116.803533	5.577485	-0.027012	2.563892
139.405283	2124.861776	5.582490	-0.027095	2.568359
139.933173	2132.917974	5.587494	-0.027199	2.572825
139.996810	2140.986867	5.592499	-0.027216	2.577258
140.315821	2149.050156	5.597504	-0.027281	2.581698
140.658128	2157.089757	5.602509	-0.027350	2.586119
140.838453	2165.188230	5.607514	-0.027388	2.590553
141.322709	2173.394250	5.612518	-0.027484	2.595059
141.706394	2181.340841	5.617523	-0.027560	2.599409
142.059247	2189.364936	5.622528	-0.027631	2.603791
142.110388	2197.414978	5.627533	-0.027646	2.608160
142.189648	2205.469868	5.632538	-0.027666	2.612526
142.620511	2213.496680	5.637542	-0.027751	2.616894
143.054964	2221.474180	5.642547	-0.027837	2.621227
143.436356	2229.529427	5.647552	-0.027914	2.625592
143.670960	2237.587976	5.652557	-0.027963	2.629941
144.030561	2245.648963	5.657562	-0.028035	2.634292
144.114655	2253.726527	5.662566	-0.028056	2.638627
144.781333	2261.677209	5.667571	-0.028185	2.642926
145.259701	2269.746523	5.672576	-0.028279	2.647268
145.399114	2277.834882	5.677581	-0.028310	2.651591
145.694339	2285.905149	5.682586	-0.028371	2.655908
146.092330	2293.940910	5.687590	-0.028450	2.660205
146.123541	2301.985187	5.692595	-0.028461	2.664477
146.721340	2310.030612	5.697600	-0.028577	2.668779
147.091734	2318.114068	5.702605	-0.028652	2.673079
147.306973	2326.162751	5.707610	-0.028697	2.677344
147.583375	2334.199216	5.712614	-0.028754	2.681600
147.908066	2342.226752	5.717619	-0.028819	2.685847
148.419819	2350.245195	5.722624	-0.028920	2.690094
148.626057	2358.350365	5.727629	-0.028963	2.694361
148.818872	2366.372339	5.732634	-0.029004	2.698577
149.277750	2374.415013	5.737638	-0.029095	2.702813
149.413339	2382.450753	5.742643	-0.029126	2.707019
149.860727	2390.509053	5.747648	-0.029214	2.711250
150.147171	2398.565854	5.752653	-0.029273	2.715463
150.426218	2406.587547	5.757658	-0.029330	2.719651
150.719212	2414.629138	5.762662	-0.029390	2.723843
151.174764	2422.656716	5.767667	-0.029480	2.728032
151.689509	2430.711000	5.772672	-0.029581	2.732232
152.186132	2438.751710	5.777677	-0.029678	2.736417
152.512776	2446.782759	5.782682	-0.029744	2.740580
153.077260	2454.810226	5.787686	-0.029855	2.744750
153.138240	2462.901155	5.792691	-0.029871	2.748915
153.312482	2471.064667	5.797696	-0.029909	2.753117
153.769926	2479.086801	5.802701	-0.029999	2.757258
153.798251	2487.117348	5.807706	-0.030010	2.761372
154.209043	2495.126049	5.812710	-0.030091	2.765491
154.594776	2503.127217	5.817715	-0.030168	2.769598
154.934470	2511.209618	5.822720	-0.030237	2.773738
155.120602	2519.250997	5.827725	-0.030277	2.777841
155.256278	2527.291811	5.832730	-0.030307	2.781935
155.709247	2535.319977	5.837734	-0.030397	2.786036
155.970925	2543.341740	5.842739	-0.030451	2.790116
156.420072	2551.402460	5.847744	-0.030539	2.794220
156.652884	2559.437856	5.852749	-0.030588	2.798293
156.939079	2567.468403	5.857754	-0.030647	2.802361
157.174888	2575.538303	5.862758	-0.030696	2.806439
157.562817	2583.555988	5.867763	-0.030773	2.810495
157.742844	2591.627404	5.872768	-0.030812	2.814559
158.037252	2599.676917	5.877773	-0.030872	2.818613
158.343355	2607.704410	5.882778	-0.030934	2.822650
158.719043	2615.757487	5.887782	-0.031009	2.826699
158.945047	2623.806874	5.892787	-0.031056	2.830731
159.202996	2631.887415	5.897792	-0.031110	2.834775
159.412054	2639.894226	5.902797	-0.031154	2.838774
159.722719	2647.902169	5.907802	-0.031217	2.842773
159.917729	2655.962991	5.912806	-0.031258	2.846787
160.058203	2663.991694	5.917811	-0.031290	2.850775
160.439571	2672.053736	5.922816	-0.031366	2.854788
160.578327	2680.094033	5.927821	-0.031397	2.858771
160.749428	2688.140722	5.932826	-0.031434	2.862754
161.087450	2696.176792	5.937830	-0.031502	2.866735
161.518781	2704.174417	5.942835	-0.031588	2.870696
161.829833	2712.251447	5.947840	-0.031651	2.874684
161.878459	2720.312573	5.952845	-0.031665	2.878645
161.893845	2728.353500	5.957850	-0.031673	2.882588
162.247896	2736.372197	5.962854	-0.031744	2.886534
162.667160	2744.378201	5.967859	-0.031828	2.890471
163.085301	2752.442828	5.972864	-0.031911	2.894432
163.256481	2760.489718	5.977869	-0.031948	2.898365
163.453191	2768.495415	5.982874	-0.031989	2.902274
163.955865	2776.547620	5.987878	-0.032088	2.906217
164.479286	2784.563078	5.992883	-0.032191	2.910138
164.773312	2792.717942	5.997888	-0.032251	2.914108
165.385582	2800.707878	6.002893	-0.032370	2.918010
165.410292	2808.738377	6.007898	-0.032380	2.921896
166.044961	2816.736122	6.012902	-0.032503	2.925792
166.195419	2824.760205	6.017907	-0.032536	2.929671
166.541885	2832.835246	6.022912	-0.032606	2.933579
166.935980	2840.853723	6.027917	-0.032685	2.937457
167.096343	2848.877197	6.032922	-0.032720	2.941320
167.447887	2856.915971	6.037926	-0.032790	2.945196
167.669318	2864.950927	6.042931	-0.032837	2.949057
167.919467	2873.029343	6.047936	-0.032889	2.952936
168.012181	2881.098896	6.052941	-0.032911	2.956797
168.097577	2889.118971	6.057946	-0.032932	2.960629
168.614961	2897.096505	6.062950	-0.033034	2.964459
168.695449	2905.156444	6.067955	-0.033054	2.968300
169.130170	2913.203395	6.072960	-0.033140	2.972147
169.369690	2921.272008	6.077965	-0.033190	2.975991
169.343980	2929.276711	6.082970	-0.033190	2.979785
169.665256	2937.321940	6.087974	-0.033255	2.983611
169.962438	2945.357116	6.092979	-0.033316	2.987427
170.356447	2953.418909	6.097984	-0.033394	2.991255
170.604277	2961.486198	6.102989	-0.033446	2.995073
170.846298	2969.480327	6.107994	-0.033496	2.998852
171.051582	2977.525062	6.112998	-0.033540	3.002647
170.895396	2985.558340	6.118003	-0.033516	3.006415
171.147628	2993.587966	6.123008	-0.033568	3.010196
171.665553	3001.620603	6.128013	-0.033669	3.013987
171.898645	3009.643425	6.133018	-0.033718	3.017755
172.314668	3017.692016	6.138022	-0.033801	3.021539
172.656598	3025.693097	6.143027	-0.033870	3.025292
172.868042	3033.733296	6.148032	-0.033914	3.029053
172.723643	3041.838034	6.153037	-0.033892	3.032821
173.032113	3049.866847	6.158042	-0.033955	3.036572
173.493639	3057.852928	6.163046	-0.034046	3.040305
173.636584	3065.867870	6.168051	-0.034078	3.044032
173.884904	3073.903406	6.173056	-0.034129	3.047768
174.275920	3081.952463	6.178061	-0.034207	3.051513
174.267881	3090.024263	6.183066	-0.034211	3.055245
174.595814	3098.049820	6.188070	-0.034277	3.058968
174.883371	3106.046798	6.193075	-0.034336	3.062670
174.884517	3114.125598	6.198080	-0.034342	3.066392
174.956966	3122.165536	6.203085	-0.034360	3.070095
175.269886	3130.251234	6.208090	-0.034424	3.073826
175.834574	3138.258050	6.213094	-0.034534	3.077528
175.394794	3146.316725	6.218099	-0.034457	3.081202
175.916719	3154.273119	6.223104	-0.034560	3.084870
176.322579	3162.298790	6.228109	-0.034640	3.088559
176.452135	3170.347777	6.233114	-0.034670	3.092242
176.658938	3178.400027	6.238118	-0.034714	3.095926
177.038575	3186.376760	6.243123	-0.034789	3.099579
177.348520	3194.418127	6.248128	-0.034852	3.103253
177.597544	3202.469790	6.253133	-0.034904	3.106925
177.779128	3210.500702	6.258138	-0.034943	3.110581
178.215669	3218.566711	6.263142	-0.035029	3.114259
178.041853	3226.603223	6.268147	-0.035002	3.117892
178.178694	3234.629229	6.273152	-0.035033	3.121530
178.464910	3242.638815	6.278157	-0.035091	3.125163
178.661484	3250.657051	6.283162	-0.035133	3.128792
178.878399	3258.728415	6.288166	-0.035179	3.132441
179.479789	3266.724275	6.293171	-0.035296	3.136069
179.578384	3274.738166	6.298176	-0.035319	3.139679
179.673501	3282.813814	6.303181	-0.035342	3.143312
179.847843	3290.840297	6.308186	-0.035380	3.146922
180.383603	3298.867251	6.313190	-0.035485	3.150544
180.463195	3306.921002	6.318195	-0.035505	3.154154
180.752088	3314.944100	6.323200	-0.035564	3.157756
181.119353	3322.967498	6.328205	-0.035638	3.161356
181.338882	3330.954358	6.333210	-0.035684	3.164930
181.599519	3339.000343	6.338214	-0.035737	3.168528
181.805496	3347.045454	6.343219	-0.035781	3.172119
182.149372	3355.085802	6.348224	-0.035850	3.175709
182.524466	3363.106408	6.353229	-0.035925	3.179288
182.479250	3371.152647	6.358234	-0.035922	3.182857
182.864026	3379.199139	6.363238	-0.035999	3.186440
183.141666	3387.215031	6.368243	-0.036056	3.190000
183.238882	3395.293256	6.373248	-0.036079	3.193577
183.591197	3403.310347	6.378253	-0.036150	3.197133
183.700040	3411.311533	6.383258	-0.036175	3.200668
183.867902	3419.344380	6.388262	-0.036212	3.204216
183.889404	3427.404322	6.393267	-0.036221	3.207765
184.216830	3435.436515	6.398272	-0.036287	3.211311
184.233083	3443.491426	6.403277	-0.036295	3.214850
184.507817	3451.476825	6.408282	-0.036352	3.218365
185.004969	3459.490137	6.413286	-0.036449	3.221898
185.008993	3467.513720	6.418291	-0.036455	3.225412
185.240134	3475.551266	6.423296	-0.036504	3.228936
185.471799	3483.659873	6.428301	-0.036552	3.232488
185.732359	3491.690367	6.433306	-0.036606	3.236003
185.976569	3499.676786	6.438310	-0.036656	3.239495
186.217451	3507.674407	6.443315	-0.036706	3.242987
186.577870	3515.677621	6.448320	-0.036779	3.246483
186.733006	3523.708584	6.453325	-0.036813	3.249978
186.839165	3531.750627	6.458330	-0.036838	3.253473
187.187375	3539.828850	6.463334	-0.036908	3.256989
187.321703	3547.824518	6.468339	-0.036938	3.260458
187.690798	3555.841228	6.473344	-0.037012	3.263940
187.804196	3563.892198	6.478349	-0.037038	3.267424
188.014873	3571.904614	6.483354	-0.037083	3.270892
188.147411	3579.969684	6.488358	-0.037112	3.274375
188.573136	3588.000868	6.493363	-0.037197	3.277851
188.727715	3595.992745	6.498368	-0.037231	3.281296
189.058983	3603.993859	6.503373	-0.037298	3.284749
189.236499	3612.034143	6.508378	-0.037336	3.288208
189.732063	3620.104634	6.513382	-0.037433	3.291689
190.008210	3628.154034	6.518387	-0.037490	3.295149
190.063005	3636.174204	6.523392	-0.037505	3.298584
190.411182	3644.205777	6.528397	-0.037575	3.302032
190.316049	3652.205730	6.533402	-0.037563	3.305445
190.562472	3660.263322	6.538406	-0.037614	3.308893
190.751508	3668.313287	6.543411	-0.037654	3.312332
191.160298	3676.325113	6.548416	-0.037736	3.315759
191.414106	3684.327550	6.553421	-0.037788	3.319172
191.528755	3692.316810	6.558426	-0.037815	3.322571
191.813007	3700.359731	6.563430	-0.037873	3.325996
192.238798	3708.334578	6.568435	-0.037957	3.329394
192.512560	3716.410732	6.573440	-0.038013	3.332825
192.706991	3724.502280	6.578445	-0.038055	3.336257
192.882416	3732.473873	6.583450	-0.038093	3.339633
192.931198	3740.546741	6.588454	-0.038107	3.343044
193.149377	3748.556170	6.593459	-0.038153	3.346431
193.630356	3756.553288	6.598464	-0.038248	3.349819
193.879374	3764.636652	6.603469	-0.038299	3.353232
193.901517	3772.666986	6.608474	-0.038308	3.356610
194.239366	3780.684961	6.613478	-0.038377	3.359991
194.548475	3788.680904	6.618483	-0.038439	3.363358
194.769595	3796.718620	6.623488	-0.038486	3.366737
195.083033	3804.749924	6.628493	-0.038549	3.370112
195.318545	3812.818471	6.633498	-0.038598	3.373497
195.625467	3820.848073	6.638502	-0.038661	3.376865
195.805052	3828.839807	6.643507	-0.038699	3.380209
196.265044	3836.874953	6.648512	-0.038790	3.383577
196.649141	3844.894765	6.653517	-0.038867	3.386934
196.538297	3852.911165	6.658522	-0.038851	3.390268
196.911423	3861.067433	6.663526	-0.038926	3.393673
196.974553	3869.049116	6.668531	-0.038943	3.396992
197.380341	3877.012978	6.673536	-0.039024	3.400313
197.522283	3885.030195	6.678541	-0.039055	3.403643
197.592607	3893.040948	6.683546	-0.039074	3.406964
197.836411	3901.064763	6.688550	-0.039124	3.410294
198.045950	3909.117511	6.693555	-0.039168	3.413631
198.187760	3917.149821	6.698560	-0.039200	3.416954
198.671802	3925.154975	6.703565	-0.039295	3.420274
198.761963	3933.194504	6.708570	-0.039317	3.423592
199.259995	3941.206870	6.713574	-0.039415	3.426909
199.578427	3949.204000	6.718579	-0.039480	3.430211
199.598019	3957.263047	6.723584	-0.039489	3.433524
199.840525	3965.324650	6.728589	-0.039539	3.436843
200.011526	3973.313958	6.733594	-0.039576	3.440127
200.407797	3981.320902	6.738598	-0.039655	3.443422
200.495260	3989.379011	6.743603	-0.039676	3.446725
200.597886	3997.386412	6.748608	-0.039701	3.450004
200.905704	4005.459084	6.753613	-0.039763	3.453314
201.164057	4013.487786	6.758618	-0.039817	3.456601
201.307120	4021.491388	6.763622	-0.039848	3.459870
201.567825	4029.513919	6.768627	-0.039902	3.463149
201.825241	4037.555949	6.773632	-0.039955	3.466431
202.033701	4045.568928	6.778637	-0.039999	3.469698
202.240763	4053.633483	6.783642	-0.040043	3.472982
202.677882	4061.642935	6.788646	-0.040130	3.476248
202.834345	4069.639177	6.793651	-0.040164	3.479496
202.898921	4077.667940	6.798656	-0.040181	3.482752
203.328079	4085.680222	6.803661	-0.040266	3.486009
203.278146	4093.692982	6.808666	-0.040262	3.489249
203.474611	4101.734865	6.813670	-0.040304	3.492504
203.895540	4109.762969	6.818675	-0.040387	3.495759
204.261538	4117.758890	6.823680	-0.040461	3.498995
204.666458	4125.813628	6.828685	-0.040541	3.502254
205.068035	4133.775460	6.833690	-0.040621	3.505472
205.761796	4141.813867	6.838694	-0.040756	3.508726
206.048730	4149.872754	6.843699	-0.040814	3.511974
206.151811	4157.903575	6.848704	-0.040839	3.515201
206.413011	4165.919586	6.853709	-0.040892	3.518424
206.710948	4173.944943	6.858714	-0.040953	3.521649
206.958684	4181.960564	6.863718	-0.041004	3.524866
207.080846	4189.977562	6.868723	-0.041032	3.528076
207.330167	4198.030576	6.873728	-0.041084	3.531302
207.359448	4206.106162	6.878733	-0.041095	3.534527
207.605593	4214.104650	6.883738	-0.041146	3.537725
207.960241	4222.136027	6.888742	-0.041217	3.540936
208.147934	4230.150532	6.893747	-0.041257	3.544132
208.210165	4238.217095	6.898752	-0.041274	3.547343
208.585487	4246.251109	6.903757	-0.041349	3.550547
208.694538	4254.354089	6.908762	-0.041375	3.553768
208.786177	4262.379165	6.913766	-0.041397	3.556954
209.078380	4270.291023	6.918771	-0.041456	3.560099
209.277043	4278.277662	6.923776	-0.041498	3.563267
209.450671	4286.358613	6.928781	-0.041536	3.566469
209.791511	4294.323205	6.933786	-0.041605	3.569628
210.060156	4302.386511	6.938790	-0.041660	3.572820
210.247772	4310.415590	6.943795	-0.041700	3.575993
210.354576	4318.396784	6.948800	-0.041725	3.579143
210.845280	4326.411055	6.953805	-0.041822	3.582314
211.179914	4334.412232	6.958810	-0.041889	3.585472
211.212381	4342.498097	6.963814	-0.041900	3.588652
211.296042	4350.542141	6.968819	-0.041921	3.591814
211.565805	4358.544113	6.973824	-0.041977	3.594962
211.724290	4366.565198	6.978829	-0.042011	3.598112
211.760037	4374.571085	6.983834	-0.042023	3.601250
212.296060	4382.526718	6.988838	-0.042128	3.604379
212.671638	4390.599965	6.993843	-0.042203	3.607547
212.824905	4398.629926	6.998848	-0.042237	3.610689
212.972243	4406.688177	7.003853	-0.042270	3.613839
213.030288	4414.723006	7.008858	-0.042286	3.616975
213.118798	4422.717815	7.013862	-0.042307	3.620093
213.481079	4430.731623	7.018867	-0.042380	3.623223
213.817459	4438.761570	7.023872	-0.042448	3.626357
213.996774	4446.800750	7.028877	-0.042486	3.629486
213.946937	4454.875781	7.033882	-0.042482	3.632621
214.127071	4462.905582	7.038886	-0.042521	3.635742
214.368788	4470.881715	7.043891	-0.042571	3.638841
214.511785	4478.941725	7.048896	-0.042603	3.641967
214.819237	4486.909447	7.053901	-0.042665	3.645059
215.119800	4494.933013	7.058906	-0.042727	3.648170
215.407568	4502.989503	7.063910	-0.042785	3.651290
215.320803	4511.016294	7.068915	-0.042774	3.654387
215.682100	4519.019358	7.073920	-0.042847	3.657483
215.827162	4527.073227	7.078925	-0.042879	3.660591
215.836581	4535.063703	7.083930	-0.042886	3.663668
216.089561	4543.089118	7.088934	-0.042938	3.666762
216.272630	4551.107449	7.093939	-0.042978	3.669849
216.404979	4559.174244	7.098944	-0.043007	3.672951
216.690586	4567.223021	7.103949	-0.043066	3.676047
216.700595	4575.187136	7.108954	-0.043073	3.679101
217.040204	4583.219111	7.113958	-0.043141	3.682186
217.181800	4591.200127	7.118963	-0.043173	3.685245
217.621109	4599.235120	7.123968	-0.043260	3.688329
217.878747	4607.288202	7.128973	-0.043313	3.691413
217.755185	4615.330663	7.133978	-0.043295	3.694481
218.195219	4623.337909	7.138982	-0.043382	3.697547
218.436574	4631.342863	7.143987	-0.043432	3.700604
218.569992	4639.355024	7.148992	-0.043462	3.703659
218.738617	4647.428209	7.153997	-0.043499	3.706735
219.063194	4655.413477	7.159002	-0.043565	3.709780
219.082850	4663.525439	7.164006	-0.043573	3.712862
219.441453	4671.557340	7.169011	-0.043645	3.715920
219.790938	4679.514261	7.174016	-0.043716	3.718946
220.259834	4687.546830	7.179021	-0.043808	3.722002
220.253305	4695.505188	7.184026	-0.043812	3.725015
220.485566	4703.510942	7.189030	-0.043861	3.728050
220.766989	4711.549954	7.194035	-0.043918	3.731095
220.940506	4719.572720	7.199040	-0.043956	3.734130
221.199299	4727.648030	7.204045	-0.044009	3.737184
221.640260	4735.615098	7.209050	-0.044096	3.740199
221.716367	4743.638994	7.214054	-0.044116	3.743224
222.079785	4751.649829	7.219059	-0.044189	3.746249
222.191158	4759.665553	7.224064	-0.044214	3.749267
222.388834	4767.762206	7.229069	-0.044256	3.752315
222.532593	4775.754112	7.234074	-0.044288	3.755320
222.875537	4783.783487	7.239078	-0.044357	3.758341
223.273013	4791.786979	7.244083	-0.044437	3.761351
223.297402	4799.781569	7.249088	-0.044446	3.764347
223.476494	4807.873213	7.254093	-0.044485	3.767380
223.762861	4815.854722	7.259098	-0.044543	3.770372
224.031132	4823.886418	7.264102	-0.044599	3.773380
224.177687	4831.955423	7.269107	-0.044631	3.776397
224.155992	4839.928105	7.274112	-0.044632	3.779372
224.467809	4847.988379	7.279117	-0.044695	3.782384
224.628096	4855.966217	7.284122	-0.044730	3.785360
224.826821	4864.002647	7.289126	-0.044773	3.788356
225.026584	4872.079057	7.294131	-0.044815	3.791365
225.144012	4880.101317	7.299136	-0.044842	3.794349
225.499523	4888.110832	7.304141	-0.044914	3.797332
225.687484	4896.078605	7.309146	-0.044954	3.800293
225.999694	4904.094237	7.314150	-0.045017	3.803272
226.132727	4912.119196	7.319155	-0.045047	3.806248
226.320959	4920.121973	7.324160	-0.045087	3.809215
226.516518	4928.164423	7.329165	-0.045129	3.812194
226.652952	4936.205698	7.334170	-0.045159	3.815169
226.731090	4944.211021	7.339174	-0.045179	3.818128
226.859078	4952.240034	7.344179	-0.045208	3.821094
227.021040	4960.218350	7.349184	-0.045243	3.824039
227.253066	4968.291276	7.354189	-0.045292	3.827019
227.276919	4976.274733	7.359194	-0.045302	3.829959
227.590674	4984.335320	7.364198	-0.045365	3.832931
227.573128	4992.372626	7.369203	-0.045367	3.835885
227.712796	5000.365603	7.374208	-0.045398	3.838825
228.217170	5008.374062	7.379213	-0.045497	3.841774
228.249083	5016.322538	7.384218	-0.045508	3.844690
228.465268	5024.422737	7.389222	-0.045554	3.847664
228.455653	5032.439515	7.394227	-0.045557	3.850599
228.589968	5040.480044	7.399232	-0.045588	3.853544
229.093106	5048.526926	7.404237	-0.045686	3.856497
229.428712	5056.474871	7.409242	-0.045754	3.859407
229.791240	5064.537846	7.414246	-0.045827	3.862358
229.869235	5072.516535	7.419251	-0.045846	3.865270
229.985718	5080.569442	7.424256	-0.045873	3.868208
230.301922	5088.656282	7.429261	-0.045937	3.871160
230.551143	5096.868903	7.434266	-0.045989	3.874154
230.786841	5104.820785	7.439270	-0.046038	3.877051
230.803102	5112.750103	7.444275	-0.046046	3.879933
231.249935	5120.731117	7.449280	-0.046135	3.882839
231.229438	5128.720822	7.454285	-0.046136	3.885738
231.263458	5136.741162	7.459290	-0.046148	3.888647
231.789052	5144.779466	7.464294	-0.046251	3.891570
231.735906	5152.793283	7.469299	-0.046246	3.894470
231.866075	5160.820704	7.474304	-0.046275	3.897376
232.094975	5168.836059	7.479309	-0.046323	3.900278
232.291999	5176.819378	7.484314	-0.046365	3.903166
232.418104	5184.840068	7.489318	-0.046394	3.906063
232.842683	5192.884247	7.494323	-0.046478	3.908973
233.190424	5200.905637	7.499328	-0.046548	3.911870
233.567473	5208.936830	7.504333	-0.046623	3.914770
233.697169	5216.912156	7.509338	-0.046653	3.917642
233.809212	5224.938588	7.514342	-0.046679	3.920531
233.977672	5232.946405	7.519347	-0.046715	3.923411
234.231646	5240.946297	7.524352	-0.046768	3.926289
234.493704	5249.009213	7.529357	-0.046822	3.929187
234.629181	5257.039253	7.534362	-0.046852	3.932068
234.788722	5265.073175	7.539366	-0.046887	3.934949
235.030508	5273.067096	7.544371	-0.046937	3.937816
235.230163	5281.062056	7.549376	-0.046980	3.940680
235.477428	5289.047469	7.554381	-0.047031	3.943539
235.775483	5297.073011	7.559386	-0.047091	3.946411
236.004199	5305.118428	7.564390	-0.047139	3.949287
236.407426	5313.170059	7.569395	-0.047220	3.952166
236.473125	5321.218727	7.574400	-0.047237	3.955036
236.796747	5329.259921	7.579405	-0.047302	3.957906
237.009528	5337.209774	7.584410	-0.047347	3.960739
237.305992	5345.195645	7.589414	-0.047408	3.963584
237.323133	5353.255221	7.594419	-0.047416	3.966449
237.316146	5361.269903	7.599424	-0.047420	3.969296
237.768262	5369.313456	7.604429	-0.047509	3.972158
237.865761	5377.311064	7.609434	-0.047533	3.974996
238.085450	5385.345703	7.614438	-0.047579	3.977847
238.373995	5393.363580	7.619443	-0.047638	3.980691
238.068907	5401.345282	7.624448	-0.047586	3.983510
238.790226	5409.369637	7.629453	-0.047725	3.986360
238.965195	5417.389074	7.634458	-0.047763	3.989196
238.997102	5425.488992	7.639462	-0.047774	3.992057
238.952130	5433.547815	7.644467	-0.047771	3.994900
239.303478	5441.534043	7.649472	-0.047842	3.997722
239.524381	5449.521363	7.654477	-0.047888	4.000540
239.552666	5457.540874	7.659482	-0.047899	4.003364
239.662474	5465.569493	7.664486	-0.047924	4.006190
240.021874	5473.575757	7.669491	-0.047996	4.009011
239.957290	5481.601431	7.674496	-0.047989	4.011830
240.413147	5489.654051	7.679501	-0.048080	4.014664
240.674886	5497.650839	7.684506	-0.048133	4.017474
240.685192	5505.657304	7.689510	-0.048141	4.020282
240.869763	5513.695599	7.694515	-0.048180	4.023101
241.159775	5521.683271	7.699520	-0.048239	4.025902
241.241580	5529.756214	7.704525	-0.048260	4.028728
241.262885	5537.771385	7.709530	-0.048269	4.031530
241.703021	5545.854539	7.714534	-0.048356	4.034361
241.888450	5553.856992	7.719539	-0.048396	4.037158
241.840787	5561.786421	7.724544	-0.048392	4.039923
242.182177	5569.818483	7.729549	-0.048461	4.042729
242.261119	5577.810914	7.734554	-0.048481	4.045515
242.487553	5585.842147	7.739558	-0.048528	4.048314
242.891024	5593.884180	7.744563	-0.048608	4.051118
242.893297	5601.902904	7.749568	-0.048614	4.053906
243.054243	5609.961909	7.754573	-0.048649	4.056708
243.377992	5617.876804	7.759578	-0.048715	4.059461
243.688529	5625.943577	7.764582	-0.048778	4.062264
243.837712	5633.935299	7.769587	-0.048811	4.065037
243.758087	5641.977033	7.774592	-0.048801	4.067822
243.987194	5650.008113	7.779597	-0.048849	4.070606
244.096710	5658.037890	7.784602	-0.048874	4.073386
244.394578	5666.056601	7.789606	-0.048935	4.076163
244.384225	5674.059799	7.794611	-0.048938	4.078928
244.598355	5682.058589	7.799616	-0.048983	4.081693
244.973055	5690.034815	7.804621	-0.049058	4.084450
245.031775	5698.078865	7.809626	-0.049074	4.087224
245.242067	5706.066273	7.814630	-0.049119	4.089980
245.547845	5714.167898	7.819635	-0.049181	4.092774
245.760363	5722.178074	7.824640	-0.049226	4.095533
245.815185	5730.198026	7.829645	-0.049241	4.098291
245.972166	5738.192219	7.834650	-0.049275	4.101041
246.111029	5746.190723	7.839654	-0.049306	4.103789
246.178377	5754.247427	7.844659	-0.049324	4.106555
246.527828	5762.251563	7.849664	-0.049394	4.109305
246.604577	5770.324339	7.854669	-0.049414	4.112072
246.720907	5778.368281	7.859674	-0.049441	4.114829
246.791754	5786.368268	7.864678	-0.049459	4.117568
247.044873	5794.350423	7.869683	-0.049511	4.120301
247.348876	5802.337941	7.874688	-0.049573	4.123035
247.331763	5810.393879	7.879693	-0.049575	4.125786
247.631479	5818.341157	7.884698	-0.049636	4.128503
247.660266	5826.404347	7.889702	-0.049647	4.131253
247.892162	5834.454601	7.894707	-0.049695	4.134001
248.066017	5842.500481	7.899712	-0.049733	4.136744
248.616165	5850.454856	7.904717	-0.049840	4.139458
248.723836	5858.502927	7.909722	-0.049866	4.142197
248.819514	5866.474127	7.914726	-0.049889	4.144908
249.084085	5874.582541	7.919731	-0.049943	4.147666
249.539661	5882.565618	7.924736	-0.050033	4.150382
249.839539	5890.623960	7.929741	-0.050094	4.153120
249.901329	5898.659134	7.934746	-0.050111	4.155845
250.167334	5906.612413	7.939750	-0.050165	4.158543
250.348851	5914.655021	7.944755	-0.050204	4.161269
250.555207	5922.629232	7.949760	-0.050248	4.163970
250.852448	5930.685063	7.954765	-0.050309	4.166697
250.808794	5938.651477	7.959770	-0.050306	4.169389
250.835318	5946.732574	7.964774	-0.050316	4.172119
251.106901	5954.723870	7.969779	-0.050372	4.174819
251.189183	5962.735038	7.974784	-0.050392	4.177522
251.464489	5970.747884	7.979789	-0.050448	4.180226
251.737704	5978.767034	7.984794	-0.050505	4.182930
251.977331	5986.763822	7.989798	-0.050554	4.185625
252.215456	5994.845754	7.994803	-0.050604	4.188346
252.385492	6002.837689	7.999808	-0.050641	4.191035
252.579015	6010.960503	8.004813	-0.050682	4.193766
252.622036	6018.961379	8.009818	-0.050695	4.196453
252.704728	6026.855402	8.014822	-0.050716	4.199102
253.112268	6034.924982	8.019827	-0.050797	4.201813
253.231237	6042.866319	8.024832	-0.050824	4.204475
253.340230	6050.948269	8.029837	-0.050850	4.207183
253.676430	6058.906273	8.034842	-0.050917	4.209850
253.631808	6066.969771	8.039846	-0.050914	4.212546
253.866111	6075.020641	8.044851	-0.050963	4.215239
253.712139	6083.001489	8.049856	-0.050940	4.217904
254.252657	6090.997452	8.054861	-0.051045	4.220578
254.484224	6098.984482	8.059866	-0.051094	4.223245
254.365510	6107.003850	8.064870	-0.051077	4.225918
254.658632	6115.091178	8.069875	-0.051137	4.228615
254.735035	6123.053165	8.074880	-0.051156	4.231267
255.011772	6131.143911	8.079885	-0.051213	4.233962
255.157692	6139.154470	8.084890	-0.051245	4.236627
255.508598	6147.139865	8.089894	-0.051316	4.239284
255.624482	6155.184090	8.094899	-0.051342	4.241957
255.415089	6163.138149	8.099904	-0.051309	4.244595
255.821217	6171.214523	8.104909	-0.051389	4.247278
256.069998	6179.208214	8.109914	-0.051441	4.249930
255.955235	6187.214190	8.114918	-0.051425	4.252581
256.313564	6195.294253	8.119923	-0.051497	4.255259
256.603200	6203.262497	8.124928	-0.051556	4.257898
256.673603	6211.306885	8.129933	-0.051574	4.260559
256.972458	6219.290687	8.134938	-0.051635	4.263200
257.290876	6227.321602	8.139942	-0.051699	4.265855
257.519574	6235.372325	8.144947	-0.051747	4.268514
257.564012	6243.379966	8.149952	-0.051761	4.271155
257.799470	6251.430264	8.154957	-0.051810	4.273811
258.119857	6259.474950	8.159962	-0.051874	4.276464
258.272293	6267.382976	8.164966	-0.051908	4.279068
258.424906	6275.480032	8.169971	-0.051942	4.281734
258.614200	6283.418862	8.174976	-0.051982	4.284346
258.787656	6291.511277	8.179981	-0.052020	4.287006
258.787554	6299.467601	8.184986	-0.052025	4.289619
259.071515	6307.507433	8.189990	-0.052083	4.292260
259.447645	6315.576750	8.194995	-0.052158	4.294909
259.489171	6323.555463	8.200000	-0.052171	4.297525
259.725984	6331.570597	8.205005	-0.052220	4.300153
259.849058	6339.611570	8.210010	-0.052248	4.302786
260.043214	6347.583304	8.215014	-0.052290	4.305396
260.268513	6355.639459	8.220019	-0.052337	4.308032
260.617759	6363.612709	8.225024	-0.052407	4.310640
260.864331	6371.713793	8.230029	-0.052458	4.313287
260.874694	6379.711493	8.235034	-0.052465	4.315897
261.055457	6387.669973	8.240038	-0.052504	4.318495
261.185176	6395.736021	8.245043	-0.052533	4.321125
261.143491	6403.693910	8.250048	-0.052531	4.323717
261.445190	6411.733393	8.255053	-0.052592	4.326337
261.600859	6419.765717	8.260058	-0.052626	4.328951
261.679128	6427.771034	8.265062	-0.052646	4.331555
261.753921	6435.811070	8.270067	-0.052665	4.334169
262.139738	6443.844565	8.275072	-0.052742	4.336781
262.134011	6451.821094	8.280077	-0.052746	4.339370
262.203051	6459.843186	8.285082	-0.052764	4.341972
262.419450	6467.815059	8.290086	-0.052810	4.344558
262.829143	6475.883231	8.295091	-0.052891	4.347175
262.932697	6483.857534	8.300096	-0.052916	4.349758
263.260818	6491.952734	8.305101	-0.052982	4.352380
263.340861	6500.012516	8.310106	-0.053002	4.354987
263.535708	6507.996641	8.315110	-0.053044	4.357569
263.689664	6515.971883	8.320115	-0.053077	4.360146
263.627671	6523.960929	8.325120	-0.053071	4.362725
263.763433	6531.954767	8.330125	-0.053102	4.365305
263.837720	6539.974901	8.335130	-0.053121	4.367892
264.136769	6547.978164	8.340134	-0.053181	4.370473
264.248098	6556.066374	8.345139	-0.053207	4.373078
264.363208	6564.054606	8.350144	-0.053234	4.375650
264.508392	6572.058694	8.355149	-0.053266	4.378226
264.848448	6580.082513	8.360154	-0.053335	4.380807
265.148176	6588.078878	8.365158	-0.053396	4.383378
265.187437	6596.106045	8.370163	-0.053408	4.385956
265.093943	6604.120806	8.375168	-0.053396	4.388528
265.382490	6612.175532	8.380173	-0.053455	4.391113
265.381056	6620.235189	8.385178	-0.053460	4.393696
265.521192	6628.214356	8.390182	-0.053491	4.396253
265.913263	6636.235010	8.395187	-0.053569	4.398823
266.117931	6644.182591	8.400192	-0.053613	4.401367
266.341126	6652.218542	8.405197	-0.053659	4.403938
266.347190	6660.261791	8.410202	-0.053666	4.406509
266.519115	6668.245524	8.415206	-0.053703	4.409060
266.781563	6676.316671	8.420211	-0.053757	4.411638
267.060413	6684.319963	8.425216	-0.053814	4.414192
267.136844	6692.408474	8.430221	-0.053833	4.416772
267.124467	6700.368828	8.435226	-0.053836	4.419308
267.193550	6708.378634	8.440230	-0.053854	4.421860
267.617599	6716.372194	8.445235	-0.053938	4.424406
267.885309	6724.369854	8.450240	-0.053993	4.426951
268.044912	6732.430746	8.455245	-0.054028	4.429515
268.145555	6740.503108	8.460250	-0.054052	4.432080
268.263454	6748.517999	8.465254	-0.054080	4.434626
268.744653	6756.553237	8.470259	-0.054174	4.437178
268.832984	6764.498179	8.475264	-0.054196	4.439699
269.015466	6772.556760	8.480269	-0.054235	4.442254
269.466640	6780.472625	8.485274	-0.054324	4.444764
269.817523	6788.501949	8.490278	-0.054395	4.447308
270.137919	6796.573906	8.495283	-0.054460	4.449863
270.272277	6804.557189	8.500288	-0.054490	4.452389
270.472464	6812.617364	8.505293	-0.054532	4.454937
270.792804	6820.615539	8.510298	-0.054597	4.457465
271.066263	6828.602134	8.515302	-0.054653	4.459988
271.040199	6836.678038	8.520307	-0.054654	4.462536
271.352025	6844.616016	8.525312	-0.054717	4.465040
271.574379	6852.690387	8.530317	-0.054763	4.467586
271.679051	6860.704349	8.535322	-0.054788	4.470111
271.758745	6868.729116	8.540326	-0.054808	4.472637
271.944407	6876.799997	8.545331	-0.054848	4.475177
272.102733	6884.761629	8.550336	-0.054883	4.477682
272.133916	6892.739043	8.555341	-0.054893	4.480189
272.560998	6900.756682	8.560346	-0.054978	4.482709
272.708731	6908.721118	8.565351	-0.055011	4.485209
272.993118	6916.819116	8.570355	-0.055069	4.487751
273.149527	6924.804540	8.575360	-0.055103	4.490255
273.514632	6932.857300	8.580365	-0.055177	4.492780
273.606877	6940.866405	8.585370	-0.055199	4.495289
273.746262	6948.880601	8.590375	-0.055230	4.497798
273.972917	6956.893575	8.595379	-0.055277	4.500306
274.077893	6964.903175	8.600384	-0.055302	4.502811
274.324216	6972.918091	8.605389	-0.055353	4.505316
274.364147	6980.956271	8.610394	-0.055366	4.507827
274.528607	6988.916921	8.615399	-0.055402	4.510312
274.839684	6997.039037	8.620403	-0.055465	4.512847
275.002071	7005.015756	8.625408	-0.055500	4.515334
275.110716	7013.032418	8.630413	-0.055526	4.517833
275.150481	7020.997921	8.635418	-0.055538	4.520314
275.266005	7028.995377	8.640423	-0.055565	4.522804
275.553012	7036.996115	8.645427	-0.055623	4.525294
275.501964	7045.016693	8.650432	-0.055619	4.527787
275.670098	7053.065381	8.655437	-0.055656	4.530289
275.818738	7061.092573	8.660442	-0.055689	4.532783
276.131016	7069.081003	8.665447	-0.055752	4.535263
276.301311	7077.141206	8.670451	-0.055789	4.537764
276.548919	7085.125929	8.675456	-0.055840	4.540241
276.763817	7093.107234	8.680461	-0.055885	4.542714
276.736532	7101.142662	8.685466	-0.055885	4.545203
276.830232	7109.162706	8.690471	-0.055908	4.547686
277.113992	7117.200372	8.695475	-0.055966	4.550173
277.197179	7125.200079	8.700480	-0.055987	4.552647
277.385866	7133.282513	8.705485	-0.056027	4.555146
277.291639	7141.274649	8.710490	-0.056015	4.557614
277.450601	7149.204290	8.715495	-0.056049	4.560062
277.534575	7157.293407	8.720499	-0.056070	4.562558
277.575148	7165.267665	8.725504	-0.056083	4.565018
277.962851	7173.346330	8.730509	-0.056160	4.567508
278.182700	7181.327740	8.735514	-0.056206	4.569967
278.156806	7189.354894	8.740519	-0.056207	4.572438
278.476129	7197.411747	8.745523	-0.056271	4.574918
278.299255	7205.363803	8.750528	-0.056244	4.577363
278.440349	7213.420824	8.755533	-0.056275	4.579840
278.555400	7221.448786	8.760538	-0.056302	4.582306
278.734042	7229.384366	8.765543	-0.056340	4.584743
278.991540	7237.477746	8.770547	-0.056393	4.587227
278.912927	7245.439794	8.775552	-0.056384	4.589669
279.345743	7253.518312	8.780557	-0.056470	4.592146
279.641144	7261.538368	8.785562	-0.056530	4.594603
279.730606	7269.579410	8.790567	-0.056552	4.597065
279.940251	7277.542032	8.795571	-0.056596	4.599502
280.225200	7285.569138	8.800576	-0.056654	4.601958
280.435215	7293.508766	8.805581	-0.056698	4.604385
280.435345	7301.585626	8.810586	-0.056704	4.606853
280.593484	7309.563508	8.815591	-0.056738	4.609290
281.043046	7317.647976	8.820595	-0.056827	4.611757
281.105425	7325.634536	8.825600	-0.056844	4.614194
281.187377	7333.665299	8.830605	-0.056864	4.616642
281.470585	7341.651284	8.835610	-0.056922	4.619076
281.566118	7349.641462	8.840615	-0.056945	4.621509
281.889885	7357.716123	8.845619	-0.057011	4.623967
281.868807	7365.692189	8.850624	-0.057012	4.626394
282.149515	7373.763210	8.855629	-0.057070	4.628848
282.297487	7381.749039	8.860634	-0.057102	4.631275
282.570962	7389.783541	8.865639	-0.057158	4.633716
282.608790	7397.808575	8.870643	-0.057171	4.636152
282.813989	7405.799095	8.875648	-0.057214	4.638577
283.085551	7413.759027	8.880653	-0.057270	4.640991
283.278984	7421.765260	8.885658	-0.057311	4.643417
283.529356	7429.798593	8.890663	-0.057363	4.645851
283.547367	7437.841764	8.895667	-0.057371	4.648286
283.606617	7445.861435	8.900672	-0.057387	4.650714
283.919826	7453.898543	8.905677	-0.057451	4.653144
284.033806	7461.903141	8.910682	-0.057477	4.655564
284.310311	7469.887746	8.915687	-0.057534	4.657977
284.448730	7477.938115	8.920691	-0.057565	4.660408
284.377671	7485.927759	8.925696	-0.057557	4.662819
284.796756	7493.917386	8.930701	-0.057640	4.665229
285.168825	7501.963924	8.935706	-0.057715	4.667655
285.116974	7509.967245	8.940711	-0.057710	4.670067
285.377759	7518.057065	8.945715	-0.057764	4.672504
285.513966	7526.095615	8.950720	-0.057795	4.674923
285.684911	7534.119892	8.955725	-0.057832	4.677338
285.874718	7542.046730	8.960730	-0.057872	4.679721
285.929694	7550.052775	8.965735	-0.057887	4.682128
286.390024	7558.017503	8.970739	-0.057978	4.684520
286.303959	7566.072651	8.975744	-0.057967	4.686939
286.598193	7574.059371	8.980749	-0.058027	4.689335
286.848269	7582.124972	8.985754	-0.058079	4.691754
287.033342	7590.131917	8.990759	-0.058119	4.694154
287.090238	7598.180729	8.995763	-0.058135	4.696566
287.099633	7606.103044	9.000768	-0.058142	4.698939
287.388744	7614.183685	9.005773	-0.058201	4.701357
287.613046	7622.180455	9.010778	-0.058248	4.703749
287.452163	7630.114780	9.015783	-0.058223	4.706122
287.874214	7638.229964	9.020787	-0.058307	4.708547
287.962910	7646.220367	9.025792	-0.058328	4.710934
288.224361	7654.276932	9.030797	-0.058382	4.713338
288.342400	7662.349082	9.035802	-0.058409	4.715747
288.443300	7670.280785	9.040807	-0.058433	4.718113
288.681095	7678.284749	9.045811	-0.058483	4.720498
288.699309	7686.322343	9.050816	-0.058491	4.722893
288.953113	7694.303265	9.055821	-0.058544	4.725269
289.015361	7702.387240	9.060826	-0.058561	4.727675
288.875904	7710.367435	9.065831	-0.058540	4.730050
289.448115	7718.433058	9.070835	-0.058651	4.732447
289.456012	7726.401800	9.075840	-0.058658	4.734815
289.599190	7734.454751	9.080845	-0.058690	4.737207
289.897624	7742.416668	9.085850	-0.058751	4.739570
289.868987	7750.486589	9.090855	-0.058751	4.741965
289.910231	7758.441308	9.095859	-0.058763	4.744324
289.816687	7766.462802	9.100864	-0.058751	4.746702
290.182663	7774.498642	9.105869	-0.058825	4.749082
290.158955	7782.537438	9.110874	-0.058825	4.751463
290.139705	7790.567658	9.115879	-0.058827	4.753840
290.350617	7798.602466	9.120883	-0.058871	4.756217
290.471012	7806.563220	9.125888	-0.058899	4.758570
290.703157	7814.534597	9.130893	-0.058947	4.760926
290.920426	7822.587002	9.135898	-0.058993	4.763304
291.054891	7830.562116	9.140903	-0.059023	4.765658
291.200749	7838.635550	9.145907	-0.059056	4.768040
291.333264	7846.583757	9.150912	-0.059085	4.770384
291.722408	7854.639893	9.155917	-0.059163	4.772758
291.742802	7862.720762	9.160922	-0.059172	4.775139
291.683416	7870.698585	9.165927	-0.059166	4.777489
292.113852	7878.671067	9.170931	-0.059251	4.779834
292.123342	7886.716126	9.175936	-0.059258	4.782201
292.193719	7894.648168	9.180941	-0.059277	4.784534
292.222901	7902.740762	9.185946	-0.059287	4.786912
292.482659	7910.674902	9.190951	-0.059341	4.789242
292.562927	7918.790116	9.195955	-0.059361	4.791625
292.602206	7926.752402	9.200960	-0.059374	4.793962
293.001314	7934.850650	9.205965	-0.059453	4.796336
293.187137	7942.823103	9.210970	-0.059493	4.798672
293.247220	7950.792263	9.215975	-0.059509	4.801008
293.566724	7958.812008	9.220979	-0.059574	4.803355
293.598472	7966.822746	9.225984	-0.059585	4.805701
293.634236	7974.816139	9.230989	-0.059597	4.808040
293.817382	7982.917247	9.235994	-0.059636	4.810408
294.078768	7990.378540	9.240999	-0.059690	4.812588
294.104039	7995.105052	9.246003	-0.059697	4.813970
294.220816	7997.429929	9.251008	-0.059721	4.814648
294.441796	7998.583422	9.256013	-0.059762	4.814984
294.698891	7999.725850	9.261018	-0.059811	4.815317
294.544259	7999.721151	9.266023	-0.059782	4.815316
294.853532	7999.758326	9.271027	-0.059840	4.815326
294.855014	7999.716665	9.276032	-0.059840	4.815313
295.071124	7999.746955	9.281037	-0.059880	4.815321
295.313314	7999.721032	9.286042	-0.059925	4.815312
295.486996	7999.986823	9.291047	-0.059958	4.815389
295.442821	7999.928374	9.296051	-0.059949	4.815372
295.240459	7999.922884	9.301056	-0.059912	4.815372
295.322298	8000.058902	9.306061	-0.059927	4.815411
295.613948	8000.041282	9.311066	-0.059981	4.815404
295.367900	8000.114159	9.316071	-0.059935	4.815427
295.386429	7999.880397	9.321075	-0.059939	4.815359
295.501621	8000.113159	9.326080	-0.059960	4.815426
295.831982	7999.956166	9.331085	-0.060022	4.815379
295.869624	7999.942891	9.336090	-0.060029	4.815375
295.844603	8000.010877	9.341095	-0.060024	4.815395
295.902528	7999.883576	9.346099	-0.060035	4.815357
295.799990	7999.875463	9.351104	-0.060015	4.815355
295.818254	7999.934546	9.356109	-0.060019	4.815372
296.065597	7999.925811	9.361114	-0.060065	4.815369
295.762227	7999.998808	9.366119	-0.060008	4.815391
295.981585	7999.864560	9.371123	-0.060049	4.815351
296.125889	8000.028335	9.376128	-0.060076	4.815398
296.163096	7999.966956	9.381133	-0.060083	4.815380
296.128255	7999.861633	9.386138	-0.060076	4.815350
296.279632	7999.868411	9.391143	-0.060104	4.815351
296.446308	7999.778180	9.396147	-0.060135	4.815324
296.229107	8000.000100	9.401152	-0.060095	4.815390
296.408286	7999.795714	9.406157	-0.060128	4.815329
296.563278	7999.877368	9.411162	-0.060157	4.815352
296.414084	7999.771220	9.416167	-0.060129	4.815322
296.496226	7999.888007	9.421171	-0.060145	4.815355
296.654706	7999.863907	9.426176	-0.060174	4.815348
296.643042	7999.888293	9.431181	-0.060172	4.815355
296.517571	7999.868043	9.436186	-0.060148	4.815350
296.700519	7999.896720	9.441191	-0.060182	4.815357
296.827952	7999.783394	9.446195	-0.060206	4.815323
296.690004	7999.877300	9.451200	-0.060180	4.815351
296.660170	7999.793435	9.456205	-0.060175	4.815327
296.869049	7999.890946	9.461210	-0.060214	4.815355
296.800219	7999.788265	9.466215	-0.060201	4.815325
296.743833	7999.880315	9.471219	-0.060190	4.815352
296.831132	7999.781288	9.476224	-0.060206	4.815323
296.696619	7999.791884	9.481229	-0.060181	4.815326
296.920902	7999.897131	9.486234	-0.060223	4.815356
296.880672	7999.871878	9.491239	-0.060216	4.815349
297.195547	7999.880295	9.496243	-0.060274	4.815350
296.936907	7999.988236	9.501248	-0.060226	4.815383
296.997470	7999.870595	9.506253	-0.060237	4.815348
297.026893	7999.840083	9.511258	-0.060243	4.815339
297.063263	7999.860990	9.516263	-0.060249	4.815345
297.133010	7999.851453	9.521267	-0.060262	4.815342
297.069708	7999.876053	9.526272	-0.060250	4.815349
297.153104	7999.896669	9.531277	-0.060266	4.815355
296.863780	7999.781787	9.536282	-0.060212	4.815323
297.041544	7999.973908	9.541287	-0.060245	4.815378
297.067068	7999.882408	9.546291	-0.060250	4.815351
296.976435	7999.878766	9.551296	-0.060233	4.815350
296.911961	7999.871282	9.556301	-0.060221	4.815349
297.322822	7999.896252	9.561306	-0.060297	4.815354
297.353933	7999.885007	9.566311	-0.060303	4.815350
297.162071	7999.805940	9.571315	-0.060267	4.815328
297.147525	7999.875169	9.576320	-0.060265	4.815349
297.418450	7999.970503	9.581325	-0.060315	4.815375
297.270902	7999.865448	9.586330	-0.060287	4.815345
297.193079	7999.876982	9.591335	-0.060273	4.815349
297.318780	7999.869440	9.596339	-0.060296	4.815346
297.154264	7999.874194	9.601344	-0.060266	4.815348
297.253150	7999.967748	9.606349	-0.060284	4.815375
297.481886	7999.871062	9.611354	-0.060327	4.815346
297.417155	7999.892432	9.616359	-0.060314	4.815352
297.303199	7999.770833	9.621363	-0.060293	4.815317
297.387826	7999.888733	9.626368	-0.060309	4.815351
297.239811	7999.879865	9.631373	-0.060281	4.815350
297.406072	7999.781076	9.636378	-0.060312	4.815320
297.401566	7999.885744	9.641383	-0.060311	4.815350
297.535099	7999.803514	9.646387	-0.060336	4.815326
297.402073	7999.876126	9.651392	-0.060311	4.815348
297.328426	7999.892004	9.656397	-0.060298	4.815353
297.283492	7999.788649	9.661402	-0.060289	4.815323
297.358281	7999.888216	9.666407	-0.060303	4.815351
297.378572	7999.884273	9.671411	-0.060307	4.815350
297.354966	7999.989693	9.676416	-0.060302	4.815381
297.298217	7999.863696	9.681421	-0.060292	4.815345
297.233829	7999.779258	9.686426	-0.060280	4.815320
297.220364	7999.891259	9.691431	-0.060277	4.815353
297.239047	7999.793233	9.696435	-0.060281	4.815324
297.480096	7999.868832	9.701440	-0.060326	4.815345
297.342424	7999.883650	9.706445	-0.060300	4.815350
297.368262	7999.829564	9.711450	-0.060305	4.815334
297.362683	7999.919250	9.716455	-0.060304	4.815360
297.545530	7999.789739	9.721459	-0.060337	4.815322
297.548053	7999.877422	9.726464	-0.060338	4.815347
297.719433	7999.910185	9.731469	-0.060370	4.815356
297.748471	7999.855082	9.736474	-0.060375	4.815340
297.422605	7999.873196	9.741479	-0.060314	4.815347
297.561498	7999.891526	9.746483	-0.060340	4.815351
297.592373	8000.104734	9.751488	-0.060346	4.815414
297.538921	7999.890076	9.756493	-0.060336	4.815351
297.747818	7999.907427	9.761498	-0.060375	4.815355
297.561320	7999.890440	9.766503	-0.060340	4.815351
297.682571	7999.874274	9.771507	-0.060363	4.815346
297.606020	7999.986300	9.776512	-0.060348	4.815379
297.672205	7999.879440	9.781517	-0.060361	4.815347
297.784474	7999.779756	9.786522	-0.060381	4.815318
297.594855	7999.973279	9.791527	-0.060346	4.815375
297.708628	7999.877895	9.796531	-0.060367	4.815347
297.715237	7999.898309	9.801536	-0.060369	4.815353
297.741124	7999.994931	9.806541	-0.060373	4.815381
297.757404	7999.767533	9.811546	-0.060376	4.815314
297.876249	8000.004644	9.816551	-0.060398	4.815383
297.909133	7999.898300	9.821555	-0.060404	4.815352
297.752574	7999.987624	9.826560	-0.060375	4.815379
297.670216	7999.887923	9.831565	-0.060360	4.815350
297.819725	7999.777099	9.836570	-0.060388	4.815317
297.902859	7999.887494	9.841575	-0.060403	4.815349
297.927395	7999.891104	9.846579	-0.060408	4.815350
297.826703	7999.992042	9.851584	-0.060389	4.815380
297.627158	7999.870091	9.856589	-0.060352	4.815345
297.871156	7999.896575	9.861594	-0.060397	4.815351
297.972149	7999.897175	9.866599	-0.060416	4.815351
297.983036	7999.908041	9.871603	-0.060418	4.815354
297.707367	7999.873543	9.876608	-0.060366	4.815345
297.662160	7999.863171	9.881613	-0.060358	4.815343
297.802074	7999.866554	9.886618	-0.060384	4.815343
297.891256	8000.015529	9.891623	-0.060401	4.815386
297.948717	7999.893560	9.896627	-0.060411	4.815350
298.084862	7999.865884	9.901632	-0.060437	4.815341
297.986965	7999.879222	9.906637	-0.060418	4.815346
297.821290	7999.781348	9.911642	-0.060387	4.815318
297.982461	7999.998852	9.916647	-0.060417	4.815381
298.011888	7999.802668	9.921651	-0.060423	4.815323
297.940554	7999.883784	9.926656	-0.060409	4.815347
297.891833	7999.896868	9.931661	-0.060400	4.815351
297.869783	7999.901844	9.936666	-0.060396	4.815353
298.003567	8000.009873	9.941671	-0.060421	4.815384
298.021310	7999.978098	9.946675	-0.060424	4.815375
298.127460	7999.867623	9.951680	-0.060444	4.815342
297.934008	7999.973438	9.956685	-0.060408	4.815374
297.888419	7999.780287	9.961690	-0.060399	4.815317
298.109416	7999.978475	9.966695	-0.060441	4.815374
298.164848	7999.792340	9.971699	-0.060451	4.815320
297.915549	7999.970980	9.976704	-0.060405	4.815373
297.940526	7999.885883	9.981709	-0.060409	4.815348
298.174030	7999.796757	9.986714	-0.060452	4.815321
298.095478	7999.882030	9.991719	-0.060438	4.815346
298.237409	7999.818108	9.996723	-0.060464	4.815327
298.255264	7999.866499	10.001728	-0.060467	4.815341
298.288138	7999.883073	10.006733	-0.060474	4.815345
298.327602	7999.783251	10.011738	-0.060481	4.815316
298.024188	7999.996267	10.016743	-0.060424	4.815380
298.087457	7999.988761	10.021747	-0.060436	4.815377
297.975133	7999.872530	10.026752	-0.060415	4.815344
298.004789	7999.865536	10.031757	-0.060421	4.815342
298.177845	7999.898327	10.036762	-0.060453	4.815350
298.014595	7999.968301	10.041767	-0.060422	4.815372
297.894857	7999.881875	10.046771	-0.060400	4.815347
298.146721	7999.988653	10.051776	-0.060447	4.815377
298.264967	7999.865553	10.056781	-0.060469	4.815340
298.403193	7999.894561	10.061786	-0.060495	4.815348
297.995118	7999.994682	10.066791	-0.060419	4.815380
298.271244	7999.853889	10.071795	-0.060470	4.815337
298.356725	7999.930121	10.076800	-0.060486	4.815359
298.060005	7999.869622	10.081805	-0.060431	4.815343
298.320140	7999.888892	10.086810	-0.060479	4.815347
298.255607	7999.980810	10.091815	-0.060467	4.815374
298.321571	7999.839741	10.096819	-0.060479	4.815333
298.154335	7999.933164	10.101824	-0.060448	4.815361
298.295499	7999.804030	10.106829	-0.060474	4.815322
297.961434	7999.799562	10.111834	-0.060412	4.815323
297.944833	7999.879447	10.116839	-0.060409	4.815346
298.198127	7999.802407	10.121843	-0.060456	4.815322
298.121850	7999.866340	10.126848	-0.060442	4.815341
298.076365	7999.867720	10.131853	-0.060433	4.815342
298.290322	7999.928979	10.136858	-0.060473	4.815359
298.204158	7999.898689	10.141863	-0.060457	4.815350
298.194652	7999.792712	10.146867	-0.060455	4.815320
298.308744	7999.890795	10.151872	-0.060476	4.815348
298.432262	7999.885356	10.156877	-0.060499	4.815345
298.301387	7999.784850	10.161882	-0.060475	4.815317
298.123935	7999.908032	10.166887	-0.060442	4.815354
298.312788	7999.881229	10.171891	-0.060477	4.815345
298.233734	8000.019936	10.176896	-0.060462	4.815386
298.094682	7999.793170	10.181901	-0.060436	4.815320
298.278333	7999.793002	10.186906	-0.060470	4.815319
298.250131	7999.886590	10.191911	-0.060465	4.815347
298.309370	7999.900394	10.196915	-0.060476	4.815350
298.483935	7999.884043	10.201920	-0.060509	4.815345
298.381109	7999.808585	10.206925	-0.060489	4.815323
298.484763	7999.819919	10.211930	-0.060509	4.815326
298.377615	7999.879065	10.216935	-0.060489	4.815344
298.283292	8000.001486	10.221939	-0.060471	4.815380
298.203905	7999.883662	10.226944	-0.060456	4.815346
298.149648	7999.921239	10.231949	-0.060446	4.815357
298.321922	7999.885610	10.236954	-0.060478	4.815346
298.232135	7999.887326	10.241959	-0.060461	4.815347
298.297373	7999.833892	10.246963	-0.060473	4.815331
298.329416	7999.945580	10.251968	-0.060479	4.815364
298.418606	7999.875441	10.256973	-0.060496	4.815343
298.425002	7999.889438	10.261978	-0.060497	4.815347
298.442371	8000.114185	10.266983	-0.060500	4.815412
298.384462	7999.922963	10.271987	-0.060489	4.815357
298.401685	7999.875146	10.276992	-0.060493	4.815343
298.312736	7999.891840	10.281997	-0.060476	4.815348
298.416779	7999.806983	10.287002	-0.060495	4.815323
298.354962	7999.998350	10.292007	-0.060484	4.815379
298.262971	7999.873903	10.297011	-0.060467	4.815343
298.381767	7999.990236	10.302016	-0.060489	4.815376
298.299524	7999.864882	10.307021	-0.060473	4.815340
298.531531	7999.881549	10.312026	-0.060517	4.815344
298.532407	7999.990584	10.317031	-0.060517	4.815376
298.511012	7999.943196	10.322035	-0.060513	4.815362
298.677512	7999.963053	10.327040	-0.060544	4.815367
298.354304	8000.015413	10.332045	-0.060483	4.815384
298.502650	7999.922738	10.337050	-0.060511	4.815356
298.515562	8000.073659	10.342055	-0.060513	4.815400
298.467992	7999.892229	10.347059	-0.060504	4.815347
298.499777	7999.957953	10.352064	-0.060510	4.815366
298.619905	7999.888326	10.357069	-0.060533	4.815345
298.699417	7999.911017	10.362074	-0.060547	4.815352
298.626901	8000.023112	10.367079	-0.060534	4.815385
298.443430	7999.919595	10.372083	-0.060500	4.815355
298.550755	7999.959849	10.377088	-0.060520	4.815367
298.403001	7999.793862	10.382093	-0.060492	4.815319
298.480986	7999.886003	10.387098	-0.060507	4.815345
298.411307	8000.040899	10.392103	-0.060494	4.815391
298.537984	7999.881597	10.397107	-0.060517	4.815344
298.440884	7999.966562	10.402112	-0.060499	4.815369
298.510419	7999.935645	10.407117	-0.060512	4.815360
298.615393	7999.794153	10.412122	-0.060531	4.815318
298.575096	7999.990153	10.417127	-0.060524	4.815375
298.629384	7999.914091	10.422131	-0.060534	4.815353
298.706874	7999.937817	10.427136	-0.060548	4.815360
298.463577	7999.808726	10.432141	-0.060503	4.815323
298.376971	7999.897072	10.437146	-0.060487	4.815349
298.561963	7999.903340	10.442151	-0.060521	4.815350
298.651186	7999.890919	10.447155	-0.060538	4.815346
298.505551	7999.778411	10.452160	-0.060511	4.815314
298.388040	7999.894035	10.457165	-0.060489	4.815348
298.529518	7999.794834	10.462170	-0.060515	4.815319
298.408853	8000.025842	10.467175	-0.060493	4.815387
298.608394	7999.782238	10.472179	-0.060530	4.815315
298.515778	7999.903619	10.477184	-0.060512	4.815350
298.544580	8000.020599	10.482189	-0.060518	4.815385
298.539569	7999.887973	10.487194	-0.060517	4.815346
298.536239	8000.008696	10.492199	-0.060516	4.815381
298.401895	7999.993640	10.497203	-0.060491	4.815377
298.482918	7999.891300	10.502208	-0.060506	4.815347
298.477227	7999.998088	10.507213	-0.060505	4.815378
298.570843	7999.875648	10.512218	-0.060522	4.815342
298.491699	7999.882884	10.517223	-0.060508	4.815345
298.571634	7999.897031	10.522227	-0.060522	4.815348
298.491296	7999.781329	10.527232	-0.060507	4.815315
298.450493	7999.979457	10.532237	-0.060500	4.815373
298.490605	7999.889265	10.537242	-0.060507	4.815346
298.594337	7999.788370	10.542247	-0.060526	4.815316
298.753453	7999.821999	10.547251	-0.060556	4.815326
298.587980	7999.913314	10.552256	-0.060525	4.815353
298.532365	7999.874979	10.557261	-0.060515	4.815342
298.826578	7999.798616	10.562266	-0.060569	4.815318
298.759122	7999.872316	10.567271	-0.060557	4.815340
298.599135	7999.893176	10.572275	-0.060527	4.815347
298.594607	7999.892029	10.577280	-0.060526	4.815347
298.524946	7999.959279	10.582285	-0.060513	4.815367
298.481392	7999.798225	10.587290	-0.060505	4.815320
298.581562	7999.884320	10.592295	-0.060524	4.815345
298.802443	7999.898666	10.597299	-0.060565	4.815348
298.591952	7999.782944	10.602304	-0.060525	4.815315
298.679749	7999.893419	10.607309	-0.060542	4.815347
298.813110	7999.800496	10.612314	-0.060567	4.815319
298.479162	7999.882606	10.617319	-0.060504	4.815345
298.637503	7999.808269	10.622323	-0.060534	4.815322
298.512818	7999.877813	10.627328	-0.060511	4.815343
298.472985	7999.993655	10.632333	-0.060503	4.815377
298.715882	7999.855518	10.637338	-0.060548	4.815335
298.589846	7999.891905	10.642343	-0.060525	4.815347
298.774781	7999.906723	10.647347	-0.060559	4.815350
298.575697	7999.862804	10.652352	-0.060522	4.815338
298.658816	7999.962514	10.657357	-0.060538	4.815367
298.792487	7999.780880	10.662362	-0.060562	4.815313
298.743231	7999.991696	10.667367	-0.060553	4.815375
298.826687	7999.860536	10.672371	-0.060569	4.815336
298.836702	7999.903453	10.677376	-0.060571	4.815349
298.754456	7999.853988	10.682381	-0.060555	4.815335
298.389273	7999.885344	10.687386	-0.060487	4.815346
298.674927	7999.866558	10.692391	-0.060540	4.815339
298.671406	7999.884667	10.697395	-0.060540	4.815344
298.736816	7999.894298	10.702400	-0.060552	4.815347
298.583206	7999.934504	10.707405	-0.060523	4.815359
298.661108	7999.848145	10.712410	-0.060537	4.815334
298.523553	7999.889686	10.717415	-0.060512	4.815346
298.719202	7999.799933	10.722419	-0.060548	4.815319
298.818882	7999.898847	10.727424	-0.060567	4.815348
298.804104	7999.892186	10.732429	-0.060564	4.815346
298.730869	7999.812942	10.737434	-0.060550	4.815323
298.708633	7999.953660	10.742439	-0.060546	4.815364
298.908440	7999.881078	10.747443	-0.060583	4.815342
298.863052	7999.922008	10.752448	-0.060575	4.815354
298.654291	7999.866171	10.757453	-0.060536	4.815339
298.955887	7999.805964	10.762458	-0.060592	4.815320
298.843231	7999.897085	10.767463	-0.060571	4.815347
298.650726	7999.964437	10.772467	-0.060535	4.815368
298.671055	7999.912396	10.777472	-0.060539	4.815352
298.696144	7999.892500	10.782477	-0.060544	4.815346
298.670236	7999.802283	10.787482	-0.060539	4.815320
298.480295	7999.953048	10.792487	-0.060503	4.815365
298.700431	7999.970588	10.797491	-0.060544	4.815369
298.622908	7999.986402	10.802496	-0.060530	4.815374
298.650497	7999.873555	10.807501	-0.060535	4.815341
298.544576	7999.814079	10.812506	-0.060515	4.815324
298.568787	7999.880746	10.817511	-0.060520	4.815344
298.621735	7999.910479	10.822515	-0.060529	4.815352
298.967080	7999.791140	10.827520	-0.060594	4.815316
299.012427	7999.866709	10.832525	-0.060602	4.815337
299.007765	7999.911521	10.837530	-0.060601	4.815350
298.877556	7999.785371	10.842535	-0.060577	4.815314
298.868811	7999.881420	10.847539	-0.060575	4.815342
298.876330	7999.911470	10.852544	-0.060577	4.815351
298.921325	7999.878008	10.857549	-0.060585	4.815341
298.944940	7999.890154	10.862554	-0.060589	4.815345
298.892794	7999.886079	10.867559	-0.060579	4.815344
298.744550	7999.800248	10.872563	-0.060552	4.815319
298.914950	7999.896059	10.877568	-0.060584	4.815346
298.840900	7999.885209	10.882573	-0.060570	4.815344
299.006007	7999.816327	10.887578	-0.060600	4.815323
298.815277	7999.900811	10.892583	-0.060565	4.815348
298.809286	7999.973391	10.897587	-0.060564	4.815370
298.834682	7999.895781	10.902592	-0.060568	4.815347
298.731299	7999.897271	10.907597	-0.060549	4.815348
298.892492	7999.801603	10.912602	-0.060579	4.815319
298.975379	7999.990025	10.917607	-0.060595	4.815374
298.810871	7999.798106	10.922611	-0.060564	4.815318
298.744481	7999.896406	10.927616	-0.060551	4.815347
299.025211	7999.870058	10.932621	-0.060604	4.815338
299.152820	7999.818725	10.937626	-0.060627	4.815323
298.857578	7999.889719	10.942631	-0.060572	4.815345
299.039198	7999.878830	10.947635	-0.060606	4.815341
299.207647	7999.798246	10.952640	-0.060637	4.815316
299.079119	7999.903000	10.957645	-0.060613	4.815348
299.047732	7999.888581	10.962650	-0.060608	4.815344
299.010851	7999.901861	10.967655	-0.060601	4.815348
299.118524	7999.812788	10.972659	-0.060621	4.815321
299.041735	7999.970774	10.977664	-0.060606	4.815368
298.947250	7999.824907	10.982669	-0.060589	4.815326
298.950653	7999.796101	10.987674	-0.060589	4.815317
298.849272	7999.988952	10.992679	-0.060570	4.815374
299.058098	7999.876971	10.997683	-0.060609	4.815340
299.012161	7999.895446	11.002688	-0.060601	4.815346
298.978716	7999.967571	11.007693	-0.060594	4.815367
298.908808	7999.903346	11.012698	-0.060581	4.815349
298.909400	7999.884112	11.017703	-0.060581	4.815343
298.970158	7999.890460	11.022707	-0.060593	4.815345
299.042316	7999.888446	11.027712	-0.060606	4.815344
299.209838	7999.990624	11.032717	-0.060637	4.815373
299.134025	7999.899578	11.037722	-0.060623	4.815346
298.941471	7999.876075	11.042727	-0.060587	4.815340
299.052108	7999.898214	11.047731	-0.060608	4.815346
299.110965	7999.878877	11.052736	-0.060619	4.815340
299.143431	7999.884756	11.057741	-0.060625	4.815342
299.076963	7999.788522	11.062746	-0.060612	4.815314
299.028634	8000.003630	11.067751	-0.060603	4.815377
299.019956	7999.870942	11.072755	-0.060602	4.815339
299.020866	7999.895538	11.077760	-0.060602	4.815346
299.033463	7999.874365	11.082765	-0.060604	4.815340
299.217713	7999.800456	11.087770	-0.060638	4.815317
299.211143	7999.978846	11.092775	-0.060637	4.815369
299.186095	7999.799925	11.097779	-0.060632	4.815317
299.223883	7999.894609	11.102784	-0.060639	4.815345
299.068843	7999.954031	11.107789	-0.060610	4.815363
298.989729	7999.892859	11.112794	-0.060596	4.815345
299.041090	7999.979217	11.117799	-0.060605	4.815370
299.054796	7999.888586	11.122803	-0.060608	4.815344
299.094233	7999.900994	11.127808	-0.060615	4.815347
299.086483	7999.884829	11.132813	-0.060613	4.815342
299.400688	7999.800247	11.137818	-0.060672	4.815316
299.180670	7999.884245	11.142823	-0.060631	4.815342
299.097121	7999.884995	11.147827	-0.060615	4.815342
299.182362	7999.812652	11.152832	-0.060631	4.815321
299.191797	7999.976343	11.157837	-0.060633	4.815369
299.115198	7999.817945	11.162842	-0.060619	4.815323
299.061477	7999.904699	11.167847	-0.060609	4.815348
299.178502	7999.823263	11.172851	-0.060630	4.815324
299.188948	7999.803124	11.177856	-0.060632	4.815318
299.099299	7999.892489	11.182861	-0.060615	4.815345
299.199547	7999.813981	11.187866	-0.060634	4.815321
298.991511	7999.887489	11.192871	-0.060595	4.815344
299.016125	7999.801315	11.197875	-0.060600	4.815318
299.296507	7999.889330	11.202880	-0.060652	4.815343
298.963082	7999.866699	11.207885	-0.060590	4.815338
299.030726	7999.821855	11.212890	-0.060602	4.815324
299.097061	7999.866774	11.217895	-0.060615	4.815337
299.068593	7999.894090	11.222899	-0.060609	4.815345
299.143677	7999.804476	11.227904	-0.060623	4.815319
299.140882	8000.004306	11.232909	-0.060623	4.815377
299.233470	7999.816646	11.237914	-0.060640	4.815322
299.103399	7999.897859	11.242919	-0.060616	4.815346
299.047425	7999.879826	11.247923	-0.060605	4.815341
299.343693	7999.934970	11.252928	-0.060660	4.815356
299.210164	7999.896412	11.257933	-0.060635	4.815345
299.088095	7999.809944	11.262938	-0.060613	4.815321
298.922910	7999.878818	11.267943	-0.060582	4.815341
299.155078	7999.916866	11.272947	-0.060625	4.815351
299.261740	7999.802122	11.277952	-0.060645	4.815317
299.266580	7999.871676	11.282957	-0.060646	4.815338
299.325186	7999.901504	11.287962	-0.060657	4.815346
299.167950	7999.877517	11.292967	-0.060627	4.815340
299.193758	7999.824497	11.297971	-0.060632	4.815324
299.131365	7999.896143	11.302976	-0.060620	4.815345
299.148330	7999.862217	11.307981	-0.060624	4.815335
299.073890	7999.797917	11.312986	-0.060610	4.815317
299.231850	7999.914900	11.317991	-0.060639	4.815350
299.363504	7999.815535	11.322995	-0.060663	4.815321
299.254126	7999.815857	11.328000	-0.060643	4.815321
298.997585	7999.900319	11.333005	-0.060595	4.815347
299.280597	7999.828046	11.338010	-0.060648	4.815325
299.354226	7999.907291	11.343015	-0.060662	4.815348
299.256680	7999.917429	11.348019	-0.060643	4.815351
299.132684	7999.790312	11.353024	-0.060620	4.815315
299.113123	7999.892596	11.358029	-0.060617	4.815345
299.067837	7999.904668	11.363034	-0.060608	4.815348
299.177287	7999.891515	11.368039	-0.060629	4.815344
299.312497	7999.906579	11.373043	-0.060654	4.815348
299.384610	7999.947319	11.378048	-0.060667	4.815359
299.332617	7999.869494	11.383053	-0.060657	4.815337
299.178842	7999.822050	11.388058	-0.060629	4.815324
299.217338	7999.984085	11.393063	-0.060636	4.815371
299.120792	7999.970723	11.398067	-0.060618	4.815367
299.307875	7999.888310	11.403072	-0.060653	4.815342
299.238966	7999.987639	11.408077	-0.060640	4.815372
299.229274	7999.890207	11.413082	-0.060638	4.815343
299.162712	7999.880549	11.418087	-0.060625	4.815341
299.352681	7999.879419	11.423091	-0.060661	4.815340
299.395682	7999.914332	11.428096	-0.060669	4.815350
299.131252	7999.984768	11.433101	-0.060619	4.815371
299.372648	7999.811331	11.438106	-0.060664	4.815320
299.339371	7999.887735	11.443111	-0.060658	4.815342
299.335689	7999.802161	11.448115	-0.060657	4.815317
299.237111	7999.920238	11.453120	-0.060639	4.815352
299.211031	7999.886667	11.458125	-0.060634	4.815342
299.366678	7999.863590	11.463130	-0.060663	4.815335
299.302238	7999.906342	11.468135	-0.060651	4.815348
299.366799	7999.889238	11.473139	-0.060663	4.815342
299.530802	7999.881264	11.478144	-0.060693	4.815339
299.424017	7999.859182	11.483149	-0.060674	4.815333
299.511077	7999.895894	11.488154	-0.060690	4.815344
299.639483	7999.908708	11.493159	-0.060714	4.815347
299.434759	7999.889278	11.498163	-0.060675	4.815342
299.403167	7999.903715	11.503168	-0.060670	4.815346
299.250421	7999.861632	11.508173	-0.060641	4.815335
299.346261	7999.889939	11.513178	-0.060659	4.815343
299.188220	7999.901211	11.518183	-0.060629	4.815347
299.435133	7999.948055	11.523187	-0.060675	4.815359
299.492616	7999.857081	11.528192	-0.060686	4.815332
299.284528	7999.893177	11.533197	-0.060647	4.815344
299.209755	7999.811769	11.538202	-0.060633	4.815321
299.263815	7999.883207	11.543207	-0.060643	4.815341
299.220826	7999.792706	11.548211	-0.060635	4.815315
299.161544	7999.933880	11.553216	-0.060624	4.815356
299.194425	7999.791192	11.558221	-0.060630	4.815315
299.503263	7999.907470	11.563226	-0.060688	4.815347
299.480926	7999.882512	11.568231	-0.060683	4.815340
299.446908	7999.871256	11.573235	-0.060677	4.815337
299.510776	7999.894758	11.578240	-0.060689	4.815343
299.273100	7999.903642	11.583245	-0.060645	4.815347
299.382375	7999.910794	11.588250	-0.060665	4.815349
299.382484	7999.887277	11.593255	-0.060665	4.815342
299.434736	7999.898828	11.598259	-0.060675	4.815345
299.434748	7999.790868	11.603264	-0.060675	4.815313
299.579138	7999.885181	11.608269	-0.060701	4.815340
299.525180	7999.814806	11.613274	-0.060691	4.815320
299.256274	7999.906545	11.618279	-0.060641	4.815348
299.300319	7999.800384	11.623283	-0.060649	4.815317
299.536151	7999.921866	11.628288	-0.060693	4.815351
299.295028	7999.890075	11.633293	-0.060648	4.815343
299.472011	7999.811770	11.638298	-0.060681	4.815319
299.548080	7999.904951	11.643303	-0.060695	4.815346
299.509481	7999.922479	11.648307	-0.060688	4.815351
299.500552	7999.846436	11.653312	-0.060686	4.815329
299.298190	7999.893316	11.658317	-0.060649	4.815344
299.609913	7999.814038	11.663322	-0.060707	4.815319
299.401167	7999.888603	11.668327	-0.060668	4.815342
299.321349	7999.803904	11.673331	-0.060653	4.815318
299.430542	7999.924356	11.678336	-0.060673	4.815352
299.514717	7999.992019	11.683341	-0.060689	4.815372
299.567638	7999.887073	11.688346	-0.060699	4.815341
299.541027	8000.012757	11.693351	-0.060694	4.815378
299.591448	7999.888529	11.698355	-0.060703	4.815341
299.543078	7999.808627	11.703360	-0.060694	4.815318
299.416028	7999.880270	11.708365	-0.060670	4.815340
299.549224	7999.819410	11.713370	-0.060695	4.815321
299.387067	7999.906505	11.718375	-0.060665	4.815347
299.486424	7999.798054	11.723379	-0.060683	4.815315
299.707556	7999.920362	11.728384	-0.060724	4.815350
299.582897	7999.877674	11.733389	-0.060701	4.815338
299.540956	7999.824600	11.738394	-0.060693	4.815323
299.527473	7999.792307	11.743399	-0.060691	4.815313
299.670789	7999.901567	11.748403	-0.060717	4.815345
299.480077	7999.913367	11.753408	-0.060682	4.815349
299.266341	7999.878823	11.758413	-0.060642	4.815340
299.529735	7999.805157	11.763418	-0.060691	4.815317
299.375063	7999.901996	11.768423	-0.060662	4.815346
299.291518	7999.796927	11.773427	-0.060647	4.815316
299.591161	7999.838231	11.778432	-0.060702	4.815326
299.494054	7999.872960	11.783437	-0.060684	4.815337
299.602775	7999.858725	11.788442	-0.060704	4.815332
299.571268	7999.900955	11.793447	-0.060699	4.815345
299.563495	7999.801417	11.798451	-0.060697	4.815316
299.669107	7999.919672	11.803456	-0.060717	4.815350
299.706284	7999.896769	11.808461	-0.060724	4.815343
299.743219	7999.905929	11.813466	-0.060730	4.815345
299.581966	7999.816673	11.818471	-0.060700	4.815320
299.437364	7999.902990	11.823475	-0.060673	4.815346
299.440325	7999.813250	11.828480	-0.060674	4.815320
299.341975	7999.873611	11.833485	-0.060656	4.815338
299.335599	7999.809370	11.838490	-0.060654	4.815319
299.343892	7999.805228	11.843495	-0.060656	4.815318
299.319148	7999.906358	11.848499	-0.060651	4.815348
299.306174	7999.818492	11.853504	-0.060649	4.815322
299.287859	7999.886593	11.858509	-0.060645	4.815342
299.383620	7999.810148	11.863514	-0.060663	4.815319
299.377042	7999.900890	11.868519	-0.060662	4.815346
299.165432	7999.910206	11.873523	-0.060622	4.815350
299.381492	7999.812240	11.878528	-0.060662	4.815320
299.419220	7999.879132	11.883533	-0.060670	4.815339
299.451117	7999.823007	11.888538	-0.060675	4.815323
299.374383	7999.927551	11.893543	-0.060661	4.815354
299.384911	7999.853969	11.898547	-0.060663	4.815332
299.352637	7999.860913	11.903552	-0.060657	4.815334
299.453065	7999.880745	11.908557	-0.060676	4.815340
299.649048	7999.823063	11.913562	-0.060712	4.815322
299.754217	7999.820527	11.918567	-0.060732	4.815321
299.439523	7999.880510	11.923571	-0.060673	4.815340
299.532339	7999.844634	11.928576	-0.060690	4.815329
299.353692	7999.799984	11.933581	-0.060657	4.815316
299.552287	7999.819304	11.938586	-0.060694	4.815321
299.455164	7999.820898	11.943591	-0.060676	4.815322
299.467440	7999.831787	11.948595	-0.060678	4.815325
299.484760	7999.823519	11.953600	-0.060681	4.815323
299.484761	7999.928266	11.958605	-0.060681	4.815353
299.587206	7999.813452	11.963610	-0.060700	4.815319
299.450178	7999.891344	11.968615	-0.060675	4.815343
299.439049	7999.815266	11.973619	-0.060672	4.815321
299.486769	7999.826742	11.978624	-0.060681	4.815324
299.506896	7999.795005	11.983629	-0.060685	4.815314
299.540687	7999.923828	11.988634	-0.060691	4.815352
299.544553	7999.792416	11.993639	-0.060692	4.815313
299.494795	7999.899545	11.998643	-0.060683	4.815345
299.677327	7999.799954	12.003648	-0.060717	4.815315
299.438952	7999.888992	12.008653	-0.060672	4.815342
299.608547	7999.825529	12.013658	-0.060704	4.815323
299.598562	7999.796500	12.018663	-0.060702	4.815314
299.414732	7999.832999	12.023667	-0.060668	4.815326
299.553595	7999.822470	12.028672	-0.060693	4.815322
299.526055	7999.921416	12.033677	-0.060688	4.815351
299.532174	7999.805006	12.038682	-0.060689	4.815317
299.560662	7999.892054	12.043687	-0.060695	4.815342
299.677549	7999.812753	12.048691	-0.060716	4.815319
299.659784	7999.828488	12.053696	-0.060713	4.815323
299.480299	7999.903538	12.058701	-0.060680	4.815346
299.571229	7999.845184	12.063706	-0.060696	4.815329
299.866755	7999.827633	12.068711	-0.060751	4.815322
299.684337	7999.910116	12.073715	-0.060717	4.815347
299.767328	7999.829184	12.078720	-0.060733	4.815323
299.762995	7999.817351	12.083725	-0.060732	4.815320
299.878453	7999.839570	12.088730	-0.060753	4.815326
299.658134	7999.822020	12.093735	-0.060712	4.815321
299.516777	7999.834638	12.098739	-0.060686	4.815326
299.948841	7999.841796	12.103744	-0.060766	4.815326
299.722195	7999.910720	12.108749	-0.060724	4.815347
299.708954	7999.838881	12.113754	-0.060722	4.815326
299.596365	7999.820978	12.118759	-0.060701	4.815321
299.759403	7999.834366	12.123763	-0.060731	4.815325
299.723009	7999.828415	12.128768	-0.060724	4.815323
299.856564	7999.896896	12.133773	-0.060749	4.815342
299.771526	7999.829212	12.138778	-0.060733	4.815323
299.441660	7999.807708	12.143783	-0.060672	4.815318
299.664554	7999.838121	12.148787	-0.060713	4.815326
299.934023	7999.825482	12.153792	-0.060763	4.815321
299.694712	7999.912367	12.158797	-0.060719	4.815348
299.692591	7999.994633	12.163802	-0.060718	4.815372
299.826183	7999.805513	12.168807	-0.060743	4.815316
299.649363	7999.897709	12.173811	-0.060710	4.815344
299.444474	7999.820557	12.178816	-0.060672	4.815322
299.470155	7999.901145	12.183821	-0.060677	4.815345
299.531434	7999.931017	12.188826	-0.060688	4.815354
299.697324	7999.810842	12.193831	-0.060719	4.815318
299.718121	7999.819734	12.198835	-0.060723	4.815321
299.865085	7999.837131	12.203840	-0.060750	4.815325
299.852063	7999.882874	12.208845	-0.060748	4.815338
299.734986	7999.829623	12.213850	-0.060726	4.815323
299.784996	7999.897788	12.218855	-0.060735	4.815343
299.739844	7999.819008	12.223859	-0.060727	4.815320
299.810621	7999.912102	12.228864	-0.060740	4.815347
299.701740	7999.807680	12.233869	-0.060719	4.815317
299.648303	7999.813205	12.238874	-0.060709	4.815319
299.715308	7999.898754	12.243879	-0.060722	4.815344
299.855420	7999.815562	12.248883	-0.060748	4.815319
299.967700	7999.862313	12.253888	-0.060769	4.815332
299.898387	7999.904985	12.258893	-0.060756	4.815345
299.718416	7999.827176	12.263898	-0.060722	4.815323
299.573024	7999.869656	12.268903	-0.060695	4.815336
299.576363	7999.888947	12.273907	-0.060696	4.815341
299.598481	7999.917102	12.278912	-0.060700	4.815350
299.495734	7999.864089	12.283917	-0.060681	4.815335
299.530797	7999.816567	12.288922	-0.060687	4.815321
299.546182	7999.889502	12.293927	-0.060690	4.815342
299.459700	7999.905167	12.298931	-0.060674	4.815347
299.809836	7999.809423	12.303936	-0.060739	4.815317
299.724562	7999.906344	12.308941	-0.060723	4.815346
299.550810	7999.915218	12.313946	-0.060691	4.815349
299.657940	7999.794069	12.318951	-0.060711	4.815313
299.644861	7999.893255	12.323955	-0.060708	4.815342
299.686698	7999.916391	12.328960	-0.060716	4.815349
299.630338	7999.881249	12.333965	-0.060705	4.815339
299.679697	7999.813655	12.338970	-0.060714	4.815319
299.628487	7999.901520	12.343975	-0.060705	4.815345
299.473084	7999.959868	12.348979	-0.060676	4.815363
299.733230	7999.841254	12.353984	-0.060724	4.815327
299.651702	7999.893344	12.358989	-0.060709	4.815342
299.647002	7999.829129	12.363994	-0.060708	4.815324
299.621072	7999.812663	12.368999	-0.060703	4.815319
299.743928	7999.914102	12.374003	-0.060726	4.815348
299.794687	7999.820878	12.379008	-0.060736	4.815321
299.562093	7999.792435	12.384013	-0.060692	4.815313
299.650635	7999.899718	12.389018	-0.060709	4.815344
299.667783	7999.895724	12.394023	-0.060712	4.815343
299.638212	7999.968983	12.399027	-0.060706	4.815365
299.745368	7999.802941	12.404032	-0.060726	4.815316
299.675827	7999.888364	12.409037	-0.060713	4.815341
299.707900	7999.886755	12.414042	-0.060719	4.815340
299.664171	7999.798378	12.419047	-0.060711	4.815315
299.727257	7999.985407	12.424051	-0.060723	4.815369
299.724559	7999.820749	12.429056	-0.060722	4.815321
299.701421	7999.979627	12.434061	-0.060718	4.815367
299.838524	7999.805529	12.439066	-0.060743	4.815316
300.037493	7999.890060	12.444071	-0.060780	4.815340
299.694585	7999.889716	12.449075	-0.060716	4.815341
299.756455	7999.795607	12.454080	-0.060728	4.815313
299.779119	7999.907144	12.459085	-0.060732	4.815346
299.844357	7999.906084	12.464090	-0.060744	4.815345
299.877826	7999.805091	12.469095	-0.060750	4.815316
300.005858	7999.917306	12.474099	-0.060774	4.815348
300.038964	7999.830202	12.479104	-0.060780	4.815322
299.920566	7999.892369	12.484109	-0.060758	4.815341
299.850400	7999.931820	12.489114	-0.060745	4.815353
299.685166	7999.864944	12.494119	-0.060714	4.815334
299.829777	7999.888716	12.499123	-0.060741	4.815340
299.908603	7999.815197	12.504128	-0.060756	4.815318
300.021460	7999.906851	12.509133	-0.060777	4.815345
299.934704	7999.835931	12.514138	-0.060761	4.815324
299.751229	7999.808302	12.519143	-0.060726	4.815317
299.904276	7999.907036	12.524147	-0.060755	4.815345
299.991680	7999.822970	12.529152	-0.060771	4.815320
299.820372	7999.904569	12.534157	-0.060739	4.815345
299.833026	7999.844917	12.539162	-0.060741	4.815327
299.702948	7999.831000	12.544167	-0.060717	4.815324
299.680022	7999.839168	12.549171	-0.060713	4.815326
299.839326	7999.849287	12.554176	-0.060742	4.815329
299.916708	7999.889046	12.559181	-0.060757	4.815340
299.749805	7999.820005	12.564186	-0.060726	4.815321
299.981228	7999.823837	12.569191	-0.060769	4.815321
300.078606	7999.906684	12.574195	-0.060787	4.815344
299.977037	7999.838725	12.579200	-0.060768	4.815325
299.855507	7999.815330	12.584205	-0.060745	4.815319
299.676479	7999.827323	12.589210	-0.060712	4.815323
299.913077	7999.826966	12.594215	-0.060756	4.815322
299.776630	7999.814012	12.599219	-0.060730	4.815319
299.732339	7999.841065	12.604224	-0.060722	4.815327
299.903465	7999.909101	12.609229	-0.060754	4.815346
299.943876	7999.830669	12.614234	-0.060761	4.815323
299.656400	7999.816281	12.619239	-0.060708	4.815320
299.774799	7999.918715	12.624243	-0.060730	4.815349
299.910922	7999.845077	12.629248	-0.060755	4.815327
299.860789	7999.812176	12.634253	-0.060746	4.815318
299.887211	7999.883157	12.639258	-0.060751	4.815338
300.008993	7999.812488	12.644263	-0.060773	4.815317
299.893398	7999.897148	12.649267	-0.060752	4.815342
300.067768	7999.831626	12.654272	-0.060784	4.815322
300.088195	7999.819134	12.659277	-0.060788	4.815319
300.025956	7999.936747	12.664282	-0.060776	4.815353
299.872600	7999.807003	12.669287	-0.060748	4.815316
299.852066	7999.820554	12.674291	-0.060744	4.815320
299.876145	7999.827363	12.679296	-0.060748	4.815322
299.676346	7999.815497	12.684301	-0.060711	4.815320
299.718015	7999.916660	12.689306	-0.060719	4.815349
299.903436	7999.822461	12.694311	-0.060753	4.815321
299.911322	7999.822588	12.699315	-0.060755	4.815321
299.856859	7999.806717	12.704320	-0.060745	4.815316
299.786821	7999.907097	12.709325	-0.060732	4.815346
299.870225	7999.850756	12.714330	-0.060747	4.815329
299.899431	7999.829859	12.719335	-0.060752	4.815323
299.948371	7999.896938	12.724339	-0.060761	4.815342
299.970579	7999.824618	12.729344	-0.060766	4.815321
299.816014	7999.890462	12.734349	-0.060737	4.815341
299.741402	7999.807986	12.739354	-0.060723	4.815317
300.029108	7999.899332	12.744359	-0.060776	4.815342
299.645976	7999.789296	12.749363	-0.060705	4.815312
299.866209	7999.898762	12.754368	-0.060746	4.815343
299.761696	7999.811515	12.759373	-0.060726	4.815318
299.896037	7999.909939	12.764378	-0.060751	4.815346
299.885866	7999.881975	12.769383	-0.060749	4.815338
299.891297	7999.894888	12.774387	-0.060750	4.815342
300.222002	7999.819131	12.779392	-0.060812	4.815318
299.920496	7999.891090	12.784397	-0.060756	4.815340
299.954066	7999.858507	12.789402	-0.060762	4.815331
299.912698	7999.851405	12.794407	-0.060754	4.815329
299.847042	7999.822522	12.799411	-0.060742	4.815321
300.075565	7999.921438	12.804416	-0.060785	4.815349
299.928399	7999.901892	12.809421	-0.060757	4.815344
300.023580	7999.826507	12.814426	-0.060775	4.815321
300.021822	7999.909848	12.819431	-0.060774	4.815345
299.952505	7999.916177	12.824435	-0.060761	4.815348
300.209118	7999.848812	12.829440	-0.060809	4.815327
299.936085	7999.825042	12.834445	-0.060758	4.815321
299.804644	7999.826067	12.839450	-0.060734	4.815322
299.876454	7999.886043	12.844455	-0.060747	4.815339
300.003442	7999.922349	12.849459	-0.060771	4.815349
299.986736	7999.815179	12.854464	-0.060768	4.815318
300.032742	7999.912139	12.859469	-0.060776	4.815346
299.971944	7999.827754	12.864474	-0.060765	4.815322
299.994062	7999.825979	12.869479	-0.060769	4.815321
300.055456	7999.822718	12.874483	-0.060780	4.815320
300.174709	7999.831104	12.879488	-0.060802	4.815322
300.105561	7999.909053	12.884493	-0.060790	4.815345
300.046199	7999.900583	12.889498	-0.060778	4.815343
299.941102	7999.807981	12.894503	-0.060759	4.815316
299.971981	7999.885450	12.899507	-0.060765	4.815339
300.035374	7999.835190	12.904512	-0.060776	4.815324
299.883246	7999.975897	12.909517	-0.060748	4.815365
299.978925	7999.885555	12.914522	-0.060766	4.815339
299.921098	7999.820459	12.919527	-0.060755	4.815320
299.860280	7999.816241	12.924531	-0.060743	4.815319
300.119255	7999.934902	12.929536	-0.060792	4.815352
300.135434	7999.796210	12.934541	-0.060795	4.815312
299.890753	7999.912936	12.939546	-0.060749	4.815347
300.019181	7999.814585	12.944551	-0.060773	4.815318
300.003808	7999.918010	12.949555	-0.060770	4.815348
299.957346	7999.824242	12.954560	-0.060761	4.815321
299.936655	7999.822827	12.959565	-0.060757	4.815321
300.113630	7999.836446	12.964570	-0.060790	4.815324
300.212902	7999.834881	12.969575	-0.060809	4.815323
300.045579	7999.900513	12.974579	-0.060778	4.815343
300.206529	7999.859353	12.979584	-0.060808	4.815330
299.948795	7999.903178	12.984589	-0.060760	4.815344
299.862345	7999.826919	12.989594	-0.060743	4.815322
299.901372	7999.814735	12.994599	-0.060751	4.815318
299.908116	7999.893942	12.999603	-0.060752	4.815341
299.875992	7999.805757	13.004608	-0.060746	4.815316
299.979728	7999.898329	13.009613	-0.060765	4.815342
299.958067	7999.829557	13.014618	-0.060761	4.815322
299.914753	7999.824560	13.019623	-0.060753	4.815321
299.918380	7999.918679	13.024627	-0.060754	4.815349
299.964723	7999.911961	13.029632	-0.060762	4.815346
300.129910	7999.895456	13.034637	-0.060793	4.815341
300.191899	7999.819520	13.039642	-0.060804	4.815318
300.117733	7999.804391	13.044647	-0.060790	4.815314
300.127681	7999.911442	13.049651	-0.060792	4.815345
300.018051	7999.818766	13.054656	-0.060772	4.815319
300.129399	7999.914671	13.059661	-0.060793	4.815346
300.151847	7999.818839	13.064666	-0.060797	4.815318
299.944526	7999.897703	13.069671	-0.060758	4.815342
299.789224	7999.792512	13.074675	-0.060729	4.815312
299.845731	7999.920643	13.079680	-0.060740	4.815350
299.851690	7999.880120	13.084685	-0.060741	4.815338
299.841372	7999.819019	13.089690	-0.060739	4.815320
299.868584	7999.821605	13.094695	-0.060744	4.815321
300.104704	7999.823377	13.099699	-0.060788	4.815320
300.113881	7999.918658	13.104704	-0.060789	4.815348
299.913393	7999.878988	13.109709	-0.060752	4.815337
299.975308	7999.831911	13.114714	-0.060763	4.815323
300.122729	7999.808698	13.119719	-0.060791	4.815316
300.025446	7999.908626	13.124723	-0.060773	4.815345
299.971264	7999.827558	13.129728	-0.060763	4.815322
299.980564	7999.820226	13.134733	-0.060764	4.815320
300.038063	7999.919514	13.139738	-0.060775	4.815348
300.071607	7999.834555	13.144743	-0.060781	4.815323
300.110438	7999.818093	13.149747	-0.060788	4.815318
300.046077	7999.838400	13.154752	-0.060776	4.815325
299.903140	7999.838165	13.159757	-0.060750	4.815325
300.020061	7999.861478	13.164762	-0.060771	4.815331
300.126555	7999.854689	13.169767	-0.060791	4.815329
300.082541	7999.840060	13.174771	-0.060783	4.815325
300.000954	7999.841911	13.179776	-0.060768	4.815326
299.858889	7999.817106	13.184781	-0.060741	4.815319
300.169704	7999.952660	13.189786	-0.060799	4.815357
299.885835	7999.835716	13.194791	-0.060746	4.815325
300.095190	7999.902248	13.199795	-0.060785	4.815343
300.078555	7999.827146	13.204800	-0.060782	4.815321
300.033523	7999.818914	13.209805	-0.060774	4.815319
300.165118	7999.878812	13.214810	-0.060798	4.815336
300.389187	7999.842974	13.219815	-0.060840	4.815324
300.158184	7999.824177	13.224819	-0.060797	4.815320
300.028406	7999.919291	13.229824	-0.060772	4.815348
300.227356	7999.852039	13.234829	-0.060809	4.815328
300.271132	7999.837796	13.239834	-0.060818	4.815323
300.111739	7999.823393	13.244839	-0.060788	4.815320
300.113196	7999.901443	13.249843	-0.060788	4.815343
300.303183	7999.835111	13.254848	-0.060823	4.815322
300.168184	7999.805078	13.259853	-0.060798	4.815314
300.154540	7999.930978	13.264858	-0.060796	4.815351
300.379982	7999.847062	13.269863	-0.060838	4.815326
300.014500	7999.814278	13.274867	-0.060769	4.815318
300.101934	7999.848859	13.279872	-0.060786	4.815327
300.182655	7999.833092	13.284877	-0.060801	4.815322
300.165923	7999.838155	13.289882	-0.060798	4.815324
300.197786	7999.844025	13.294887	-0.060803	4.815326
300.297772	7999.825370	13.299891	-0.060822	4.815320
300.278683	7999.875288	13.304896	-0.060818	4.815334
300.116903	7999.839467	13.309901	-0.060788	4.815325
300.093282	7999.941686	13.314906	-0.060784	4.815355
300.242660	7999.823373	13.319911	-0.060812	4.815319
299.948351	7999.800320	13.324915	-0.060757	4.815314
299.976797	7999.846750	13.329920	-0.060762	4.815327
299.906093	7999.815646	13.334925	-0.060749	4.815319
299.986398	7999.843696	13.339930	-0.060764	4.815326
300.113719	7999.934521	13.344935	-0.060787	4.815352
299.923934	7999.815931	13.349939	-0.060752	4.815319
299.933811	7999.838538	13.354944	-0.060754	4.815325
299.798194	7999.812771	13.359949	-0.060729	4.815318
299.895890	7999.924483	13.364954	-0.060747	4.815350
300.225963	7999.819855	13.369959	-0.060808	4.815318
300.036108	7999.811360	13.374963	-0.060773	4.815317
299.934483	7999.834256	13.379968	-0.060754	4.815324
299.950573	7999.840933	13.384973	-0.060757	4.815326
300.123932	7999.847010	13.389978	-0.060789	4.815327
300.141983	7999.869752	13.394983	-0.060792	4.815333
300.033543	7999.818782	13.399987	-0.060772	4.815319
299.989170	7999.951655	13.404992	-0.060764	4.815358
299.955968	7999.827109	13.409997	-0.060758	4.815322
299.787302	7999.827517	13.415002	-0.060726	4.815323
299.989239	7999.850100	13.420007	-0.060764	4.815328
300.131395	7999.826800	13.425011	-0.060790	4.815321
300.122675	7999.848030	13.430016	-0.060788	4.815327
300.097972	7999.907475	13.435021	-0.060784	4.815345
300.063322	7999.852383	13.440026	-0.060777	4.815329
299.879166	7999.839707	13.445031	-0.060743	4.815326
299.898025	7999.796192	13.450035	-0.060746	4.815313
300.049473	7999.835041	13.455040	-0.060775	4.815324
300.050933	7999.912022	13.460045	-0.060775	4.815346
299.823564	7999.820601	13.465050	-0.060732	4.815321
299.955959	7999.823861	13.470055	-0.060757	4.815321
300.097445	7999.909576	13.475059	-0.060783	4.815345
300.066634	7999.812861	13.480064	-0.060778	4.815317
300.131637	7999.909067	13.485069	-0.060790	4.815345
300.029627	7999.825068	13.490074	-0.060771	4.815321
299.910765	7999.817750	13.495079	-0.060748	4.815319
299.749603	7999.882415	13.500083	-0.060718	4.815339
300.026766	7999.924417	13.505088	-0.060770	4.815350
300.204264	7999.818329	13.510093	-0.060803	4.815318
299.977030	7999.912897	13.515098	-0.060761	4.815347
299.970028	7999.877503	13.520103	-0.060759	4.815336
300.074479	7999.885645	13.525107	-0.060779	4.815338
299.992982	7999.816950	13.530112	-0.060763	4.815319
299.999352	7999.830948	13.535117	-0.060765	4.815323
300.160919	7999.935168	13.540122	-0.060795	4.815352
300.195960	7999.826718	13.545127	-0.060801	4.815321
300.220376	7999.812155	13.550131	-0.060806	4.815316
300.180636	7999.848904	13.555136	-0.060798	4.815327
300.206534	7999.830089	13.560141	-0.060803	4.815321
299.993711	7999.856487	13.565146	-0.060763	4.815330
300.187722	7999.883215	13.570151	-0.060799	4.815337
300.103387	7999.883952	13.575155	-0.060784	4.815338
300.105760	7999.834818	13.580160	-0.060784	4.815323
300.152286	7999.828104	13.585165	-0.060793	4.815321
300.287414	7999.844236	13.590170	-0.060818	4.815325
300.262146	7999.825642	13.595175	-0.060813	4.815320
300.191647	7999.900362	13.600179	-0.060800	4.815342
300.287135	7999.849565	13.605184	-0.060818	4.815327
300.331752	7999.819304	13.610189	-0.060826	4.815318
300.298303	7999.907464	13.615194	-0.060820	4.815344
300.435294	7999.840253	13.620199	-0.060845	4.815323
300.019656	7999.825877	13.625203	-0.060768	4.815321
300.069180	7999.838453	13.630208	-0.060777	4.815325
299.925902	7999.815765	13.635213	-0.060750	4.815319
300.122349	7999.932321	13.640218	-0.060787	4.815352
300.058542	7999.831852	13.645223	-0.060775	4.815323
300.113627	7999.819935	13.650227	-0.060785	4.815319
300.240259	7999.853029	13.655232	-0.060809	4.815328
300.253249	7999.839345	13.660237	-0.060811	4.815324
300.053675	7999.823207	13.665242	-0.060774	4.815320
300.161034	7999.936148	13.670247	-0.060794	4.815353
300.176255	7999.816681	13.675251	-0.060796	4.815318
300.104472	7999.816556	13.680256	-0.060783	4.815318
300.168284	7999.833644	13.685261	-0.060795	4.815323
300.331828	7999.904761	13.690266	-0.060825	4.815343
300.282481	7999.834461	13.695271	-0.060816	4.815322
300.140076	7999.906920	13.700275	-0.060790	4.815344
300.197230	7999.842661	13.705280	-0.060800	4.815325
300.391345	7999.794568	13.710285	-0.060836	4.815310
300.394553	7999.911128	13.715290	-0.060837	4.815344
300.140179	7999.833153	13.720295	-0.060789	4.815323
300.226954	7999.898722	13.725299	-0.060806	4.815341
300.236696	7999.825126	13.730304	-0.060807	4.815320
300.235971	7999.822973	13.735309	-0.060807	4.815319
300.435303	7999.916062	13.740314	-0.060844	4.815345
300.471623	7999.831148	13.745319	-0.060851	4.815321
300.222399	7999.793878	13.750323	-0.060804	4.815311
300.215618	7999.830104	13.755328	-0.060803	4.815321
300.317169	7999.918365	13.760333	-0.060822	4.815347
300.346438	7999.819439	13.765338	-0.060827	4.815318
300.420797	7999.832426	13.770343	-0.060841	4.815321
300.221829	7999.815229	13.775347	-0.060804	4.815317
300.304338	7999.834764	13.780352	-0.060819	4.815322
300.200861	7999.825563	13.785357	-0.060800	4.815320
300.343765	7999.842893	13.790362	-0.060827	4.815325
300.392432	7999.950587	13.795367	-0.060836	4.815356
300.311634	7999.891523	13.800371	-0.060821	4.815339
300.433064	7999.846501	13.805376	-0.060843	4.815325
300.256251	7999.839291	13.810381	-0.060810	4.815324
300.226466	7999.838793	13.815386	-0.060805	4.815324
300.314372	7999.850936	13.820391	-0.060821	4.815327
300.193205	7999.828615	13.825395	-0.060798	4.815321
300.315529	7999.849879	13.830400	-0.060821	4.815327
300.278117	7999.842842	13.835405	-0.060814	4.815325
300.255611	7999.836052	13.840410	-0.060810	4.815323
300.353774	7999.851572	13.845415	-0.060828	4.815327
300.193140	7999.817907	13.850419	-0.060798	4.815318
300.286311	7999.934890	13.855424	-0.060816	4.815352
300.389752	7999.850020	13.860429	-0.060835	4.815326
300.342654	7999.840685	13.865434	-0.060826	4.815324
300.460054	7999.839421	13.870439	-0.060848	4.815323
300.410292	7999.805456	13.875443	-0.060838	4.815313
300.464535	7999.929276	13.880448	-0.060849	4.815349
300.508250	7999.819900	13.885453	-0.060857	4.815317
300.258367	7999.821099	13.890458	-0.060810	4.815319
300.256780	7999.832827	13.895463	-0.060810	4.815322
300.279232	7999.900536	13.900467	-0.060814	4.815342
300.312843	7999.908572	13.905472	-0.060820	4.815344
300.301679	7999.812183	13.910477	-0.060818	4.815316
300.163709	7999.830201	13.915482	-0.060792	4.815322
300.199393	7999.822238	13.920487	-0.060799	4.815319
300.219685	7999.900600	13.925491	-0.060803	4.815342
300.340644	7999.833124	13.930496	-0.060825	4.815322
300.243896	7999.914890	13.935501	-0.060807	4.815346
300.304044	7999.796168	13.940506	-0.060818	4.815311
300.489383	7999.927505	13.945511	-0.060853	4.815349
300.484549	7999.789533	13.950515	-0.060852	4.815308
300.247917	7999.919219	13.955520	-0.060808	4.815347
300.296108	7999.825951	13.960525	-0.060817	4.815320
300.303519	7999.842104	13.965530	-0.060818	4.815325
300.411911	7999.847104	13.970535	-0.060838	4.815326
300.285740	7999.824700	13.975539	-0.060814	4.815320
300.571941	7999.934194	13.980544	-0.060868	4.815350
300.293708	7999.808792	13.985549	-0.060816	4.815315
300.123725	7999.893620	13.990554	-0.060784	4.815340
300.411573	7999.824634	13.995559	-0.060838	4.815319
300.165379	7999.894303	14.000563	-0.060792	4.815340
300.115389	7999.820786	14.005568	-0.060783	4.815319
300.387821	7999.814610	14.010573	-0.060833	4.815316
300.375315	7999.914876	14.015578	-0.060831	4.815345
300.190238	7999.828430	14.020583	-0.060796	4.815321
300.308439	7999.890244	14.025587	-0.060818	4.815339
300.354160	7999.836485	14.030592	-0.060827	4.815323
300.365018	7999.818490	14.035597	-0.060829	4.815317
300.082265	7999.846935	14.040602	-0.060776	4.815327
300.231191	7999.895363	14.045607	-0.060804	4.815340
300.283442	7999.891950	14.050611	-0.060814	4.815339
300.222539	7999.830010	14.055616	-0.060802	4.815321
300.388541	7999.834896	14.060621	-0.060833	4.815322
300.165214	7999.831190	14.065626	-0.060791	4.815322
300.331052	7999.853176	14.070631	-0.060822	4.815328
300.414407	7999.930447	14.075635	-0.060838	4.815350
300.307880	7999.842096	14.080640	-0.060818	4.815325
300.282615	7999.807469	14.085645	-0.060813	4.815315
300.057005	7999.902064	14.090650	-0.060771	4.815343
300.067859	7999.825280	14.095655	-0.060773	4.815321
300.233198	7999.899634	14.100659	-0.060804	4.815342
300.233771	7999.810921	14.105664	-0.060804	4.815316
300.268662	7999.917317	14.110669	-0.060810	4.815347
300.276612	7999.876827	14.115674	-0.060812	4.815335
300.460514	7999.820014	14.120679	-0.060846	4.815317
300.244376	7999.895526	14.125683	-0.060806	4.815340
300.291516	7999.878133	14.130688	-0.060814	4.815335
300.447211	7999.901020	14.135693	-0.060843	4.815341
300.404403	7999.901375	14.140698	-0.060835	4.815341
300.532307	7999.825463	14.145703	-0.060859	4.815319
300.326913	7999.885119	14.150707	-0.060821	4.815337
300.402316	7999.824369	14.155712	-0.060835	4.815319
300.241674	7999.920041	14.160717	-0.060805	4.815348
300.261393	7999.810268	14.165722	-0.060808	4.815316
300.441047	7999.836759	14.170727	-0.060842	4.815322
300.283890	7999.910042	14.175731	-0.060813	4.815345
300.218428	7999.818097	14.180736	-0.060800	4.815318
300.382084	7999.917007	14.185741	-0.060831	4.815346
300.279913	7999.901414	14.190746	-0.060812	4.815342
300.500240	7999.827034	14.195751	-0.060853	4.815319
300.602217	7999.913165	14.200755	-0.060872	4.815344
300.436489	7999.845210	14.205760	-0.060841	4.815325
300.398325	7999.850987	14.210765	-0.060834	4.815327
300.488457	7999.825756	14.215770	-0.060850	4.815319
300.615826	7999.827864	14.220775	-0.060874	4.815319
300.404273	7999.903452	14.225779	-0.060835	4.815342
300.337419	7999.834999	14.230784	-0.060822	4.815322
300.420748	7999.927234	14.235789	-0.060838	4.815349
300.506685	7999.835661	14.240794	-0.060854	4.815322
300.517045	7999.840104	14.245799	-0.060855	4.815323
300.428661	7999.560724	14.250803	-0.060839	4.815242
300.569620	7996.383428	14.255808	-0.060863	4.814313
300.425535	7990.790688	14.260813	-0.060832	4.812680
300.243866	7983.944493	14.265818	-0.060794	4.810679
300.325063	7976.674194	14.270823	-0.060804	4.808553
300.012630	7969.051978	14.275827	-0.060741	4.806324
300.024623	7961.194293	14.280832	-0.060738	4.804024
300.094349	7953.383903	14.285837	-0.060746	4.801737
300.252765	7945.338865	14.290842	-0.060770	4.799379
300.190606	7937.439223	14.295847	-0.060754	4.797064
300.252624	7929.405849	14.300851	-0.060760	4.794708
300.245143	7921.386027	14.305856	-0.060753	4.792355
299.975236	7913.372734	14.310861	-0.060698	4.790004
299.928088	7905.383674	14.315866	-0.060684	4.787657
300.028711	7897.405951	14.320871	-0.060697	4.785313
299.937067	7889.397585	14.325875	-0.060675	4.782959
299.975263	7881.388618	14.330880	-0.060677	4.780603
299.970724	7873.433926	14.335885	-0.060671	4.778262
299.974165	7865.369817	14.340890	-0.060666	4.775888
299.659335	7857.422101	14.345895	-0.060602	4.773548
299.694498	7849.336788	14.350899	-0.060603	4.771165
299.889800	7841.412096	14.355904	-0.060635	4.768827
299.826412	7833.362074	14.360909	-0.060617	4.766453
299.579789	7825.365649	14.365914	-0.060566	4.764093
299.651174	7817.447972	14.370919	-0.060574	4.761755
299.542950	7809.311222	14.375923	-0.060549	4.759351
299.558774	7801.414502	14.380928	-0.060547	4.757017
299.578097	7793.348619	14.385933	-0.060545	4.754632
299.294665	7785.307601	14.390938	-0.060487	4.752253
299.382029	7777.278037	14.395943	-0.060498	4.749876
299.501164	7769.303400	14.400947	-0.060515	4.747513
299.465873	7761.324708	14.405952	-0.060503	4.745149
299.418843	7753.414106	14.410957	-0.060489	4.742804
299.323707	7745.355425	14.415962	-0.060466	4.740414
299.308083	7737.341630	14.420967	-0.060458	4.738035
299.168875	7729.307510	14.425971	-0.060427	4.735650
299.090182	7721.326422	14.430976	-0.060407	4.733279
299.425465	7713.288258	14.435981	-0.060464	4.730889
299.225675	7705.331896	14.440986	-0.060422	4.728524
298.983651	7697.301583	14.445991	-0.060371	4.726135
298.992721	7689.260929	14.450995	-0.060368	4.723741
299.063667	7681.319221	14.456000	-0.060376	4.721376
299.151011	7673.303060	14.461005	-0.060387	4.718987
299.026926	7665.341485	14.466010	-0.060358	4.716613
299.051254	7657.320329	14.471015	-0.060358	4.714221
298.863119	7649.282701	14.476019	-0.060317	4.711822
298.918660	7641.258487	14.481024	-0.060322	4.709426
299.265822	7633.314769	14.486029	-0.060382	4.707052
298.871780	7625.258680	14.491034	-0.060303	4.704645
298.877965	7617.361137	14.496039	-0.060299	4.702283
298.729552	7609.292258	14.501043	-0.060266	4.699869
298.770256	7601.315439	14.506048	-0.060268	4.697481
298.669280	7593.338588	14.511053	-0.060244	4.695092
298.618358	7585.259933	14.516058	-0.060230	4.692672
299.012479	7577.252843	14.521063	-0.060298	4.690270
298.881643	7569.289141	14.526067	-0.060268	4.687882
298.699044	7561.219013	14.531072	-0.060229	4.685460
298.755659	7553.307310	14.536077	-0.060234	4.683084
298.658215	7545.279278	14.541082	-0.060211	4.680672
298.733587	7537.360195	14.546087	-0.060220	4.678292
298.580843	7529.256093	14.551091	-0.060186	4.675855
298.523396	7521.200326	14.556096	-0.060170	4.673431
298.463031	7513.154975	14.561101	-0.060153	4.671009
298.498869	7505.176444	14.566106	-0.060155	4.668605
298.471672	7497.213130	14.571111	-0.060144	4.666206
298.336121	7489.226562	14.576115	-0.060114	4.663798
298.345966	7481.241661	14.581120	-0.060111	4.661389
298.319311	7473.235935	14.586125	-0.060100	4.658972
298.246751	7465.246617	14.591130	-0.060082	4.656559
298.184350	7457.213994	14.596135	-0.060065	4.654132
298.162005	7449.204308	14.601139	-0.060055	4.651711
298.284132	7441.175517	14.606144	-0.060073	4.649282
298.126565	7433.229498	14.611149	-0.060038	4.646878
298.031447	7425.210516	14.616154	-0.060015	4.644450
298.190043	7417.248943	14.621159	-0.060040	4.642038
297.986670	7409.201045	14.626163	-0.059996	4.639599
297.844125	7401.236841	14.631168	-0.059965	4.637183
297.856576	7393.195878	14.636173	-0.059962	4.634744
297.741148	7385.171275	14.641178	-0.059935	4.632307
297.817769	7377.157400	14.646183	-0.059944	4.629873
297.714565	7369.173158	14.651187	-0.059919	4.627447
297.761388	7361.169711	14.656192	-0.059923	4.625013
297.783498	7353.213534	14.661197	-0.059922	4.622593
297.901324	7345.178536	14.666202	-0.059938	4.620147
297.795930	7337.198880	14.671207	-0.059914	4.617717
297.799488	7329.176392	14.676211	-0.059909	4.615272
297.682504	7321.162239	14.681216	-0.059882	4.612829
297.675730	7313.157497	14.686221	-0.059875	4.610387
297.602406	7305.169295	14.691226	-0.059857	4.607949
297.605274	7297.156705	14.696231	-0.059852	4.605503
297.481594	7289.177064	14.701235	-0.059824	4.603065
297.572387	7281.148437	14.706240	-0.059835	4.600610
297.502059	7273.209953	14.711245	-0.059817	4.598182
297.268496	7265.135141	14.716250	-0.059768	4.595711
297.306265	7257.128613	14.721255	-0.059770	4.593260
297.271643	7249.078582	14.726259	-0.059758	4.590794
297.117402	7241.117633	14.731264	-0.059724	4.588354
297.154003	7233.078170	14.736269	-0.059726	4.585888
297.071979	7225.142969	14.741274	-0.059705	4.583453
296.967570	7217.121596	14.746279	-0.059681	4.580991
296.907764	7209.103454	14.751283	-0.059664	4.578528
297.180383	7201.117175	14.756288	-0.059710	4.576074
297.207610	7193.151035	14.761293	-0.059709	4.573624
297.103536	7185.086097	14.766298	-0.059685	4.571143
297.201415	7177.114137	14.771303	-0.059698	4.568689
297.119055	7169.095386	14.776307	-0.059677	4.566219
297.037320	7161.085063	14.781312	-0.059657	4.563750
296.847671	7153.143311	14.786317	-0.059616	4.561302
296.935065	7145.127874	14.791322	-0.059627	4.558829
296.909734	7137.162750	14.796327	-0.059617	4.556370
296.677359	7129.077557	14.801331	-0.059569	4.553873
296.980281	7121.086300	14.806336	-0.059620	4.551404
297.052948	7113.094339	14.811341	-0.059628	4.548933
296.797212	7105.089200	14.816346	-0.059575	4.546457
296.782317	7097.084234	14.821351	-0.059567	4.543979
296.834378	7089.118558	14.826355	-0.059572	4.541512
296.648098	7081.127321	14.831360	-0.059532	4.539036
296.825794	7073.135373	14.836365	-0.059560	4.536559
296.738025	7065.067832	14.841370	-0.059538	4.534056
296.754347	7057.088614	14.846375	-0.059536	4.531580
296.653327	7049.064261	14.851379	-0.059512	4.529088
296.512896	7041.094860	14.856384	-0.059480	4.526611
296.621586	7033.155291	14.861389	-0.059495	4.524143
296.703678	7025.134914	14.866394	-0.059505	4.521649
296.531709	7017.126789	14.871399	-0.059468	4.519156
296.528643	7009.147967	14.876403	-0.059462	4.516672
296.547158	7001.081217	14.881408	-0.059460	4.514159
296.619370	6992.994512	14.886413	-0.059469	4.511638
296.360720	6985.021022	14.891418	-0.059415	4.509150
296.507535	6977.034721	14.896423	-0.059437	4.506658
296.363734	6969.025237	14.901427	-0.059405	4.504157
296.232635	6961.069109	14.906432	-0.059376	4.501671
296.276785	6953.080953	14.911437	-0.059379	4.499174
296.018219	6945.061018	14.916442	-0.059325	4.496665
296.240464	6937.073182	14.921447	-0.059361	4.494166
295.948749	6929.025739	14.926451	-0.059302	4.491645
296.074046	6921.041717	14.931456	-0.059320	4.489144
296.044407	6913.057639	14.936461	-0.059309	4.486641
296.160595	6905.041760	14.941466	-0.059325	4.484127
296.050272	6897.055506	14.946471	-0.059300	4.481621
295.926191	6889.048070	14.951475	-0.059271	4.479106
295.815638	6881.052993	14.956480	-0.059245	4.476594
295.962190	6873.036869	14.961485	-0.059267	4.474074
295.903173	6864.957991	14.966490	-0.059251	4.471533
295.794426	6857.023130	14.971495	-0.059226	4.469035
295.775877	6849.044162	14.976499	-0.059217	4.466523
295.928132	6840.970660	14.981504	-0.059240	4.463979
295.966801	6833.028768	14.986509	-0.059242	4.461476
295.630931	6825.029475	14.991514	-0.059174	4.458951
295.625035	6817.050652	14.996519	-0.059168	4.456433
295.569315	6808.988008	15.001523	-0.059152	4.453887
295.611976	6800.976195	15.006528	-0.059155	4.451356
295.613332	6792.961554	15.011533	-0.059150	4.448822
295.457560	6785.003825	15.016538	-0.059116	4.446304
295.490266	6777.021592	15.021543	-0.059116	4.443778
295.656080	6769.041148	15.026547	-0.059142	4.441251
295.741415	6761.000274	15.031552	-0.059153	4.438703
295.590666	6753.022332	15.036557	-0.059119	4.436173
295.483879	6744.953952	15.041562	-0.059094	4.433613
295.559971	6736.919188	15.046567	-0.059103	4.431063
295.235987	6728.951703	15.051571	-0.059038	4.428531
295.151218	6720.940291	15.056576	-0.059017	4.425985
295.303104	6712.987012	15.061581	-0.059040	4.423457
295.125915	6704.950874	15.066586	-0.059001	4.420899
295.087968	6696.989934	15.071591	-0.058989	4.418365
295.142956	6688.989061	15.076595	-0.058994	4.415817
295.161302	6680.917949	15.081600	-0.058992	4.413244
295.239547	6672.941635	15.086605	-0.059001	4.410701
295.056768	6664.968138	15.091610	-0.058962	4.408156
295.130462	6656.929741	15.096615	-0.058971	4.405590
295.015939	6648.968410	15.101619	-0.058944	4.403046
294.931319	6640.974140	15.106624	-0.058923	4.400491
295.164046	6633.015424	15.111629	-0.058961	4.397947
294.888927	6624.986810	15.116634	-0.058905	4.395376
294.769886	6616.969146	15.121639	-0.058877	4.392808
294.718143	6608.945334	15.126643	-0.058862	4.390237
294.658150	6600.958522	15.131648	-0.058846	4.387676
294.757619	6592.951236	15.136653	-0.058859	4.385109
294.778623	6584.966529	15.141658	-0.058858	4.382546
294.710508	6576.987112	15.146663	-0.058840	4.379983
294.632452	6569.026179	15.151667	-0.058820	4.377425
294.692928	6560.947036	15.156672	-0.058826	4.374827
294.628089	6552.944841	15.161677	-0.058809	4.372253
294.504726	6544.919396	15.166682	-0.058781	4.369669
294.396951	6536.983736	15.171687	-0.058755	4.367112
294.444287	6528.938450	15.176691	-0.058759	4.364520
294.252277	6521.027392	15.181696	-0.058718	4.361967
294.465380	6512.994202	15.186701	-0.058752	4.359377
294.210505	6505.020325	15.191706	-0.058700	4.356801
294.317307	6496.938799	15.196711	-0.058714	4.354191
294.350592	6488.828795	15.201715	-0.058715	4.351569
294.242049	6480.895410	15.206720	-0.058690	4.349003
294.260246	6472.934278	15.211725	-0.058688	4.346427
294.321130	6464.910483	15.216730	-0.058694	4.343829
294.129458	6456.947772	15.221735	-0.058653	4.341247
293.989949	6448.969534	15.226739	-0.058622	4.338660
294.017785	6440.941585	15.231744	-0.058622	4.336056
293.991383	6432.923461	15.236749	-0.058611	4.333453
293.799363	6424.895485	15.241754	-0.058570	4.330844
293.864375	6416.927344	15.246759	-0.058577	4.328255
293.954577	6408.910612	15.251763	-0.058589	4.325649
293.807878	6400.935580	15.256768	-0.058556	4.323053
293.673805	6392.953621	15.261773	-0.058526	4.320453
293.645981	6384.959763	15.266778	-0.058516	4.317849
293.809184	6376.931940	15.271783	-0.058541	4.315233
293.699030	6368.919973	15.276787	-0.058515	4.312619
293.795483	6360.861284	15.281792	-0.058528	4.309990
293.837038	6352.940652	15.286797	-0.058530	4.307404
293.669539	6344.860616	15.291802	-0.058494	4.304762
293.687664	6336.942541	15.296807	-0.058492	4.302173
293.784899	6328.914772	15.301811	-0.058505	4.299548
293.634281	6320.929305	15.306816	-0.058471	4.296933
293.732114	6312.910343	15.311821	-0.058484	4.294307
293.610105	6304.879731	15.316826	-0.058456	4.291674
293.639041	6296.897014	15.321831	-0.058457	4.289056
293.430167	6288.893690	15.326835	-0.058412	4.286428
293.507644	6280.874890	15.331840	-0.058422	4.283795
293.410121	6272.951852	15.336845	-0.058398	4.281191
293.200388	6264.924516	15.341850	-0.058354	4.278550
293.338540	6256.905649	15.346855	-0.058374	4.275913
293.327483	6248.867089	15.351859	-0.058367	4.273267
293.213863	6240.820079	15.356864	-0.058341	4.270616
293.244919	6232.905011	15.361869	-0.058341	4.268007
293.294958	6224.828660	15.366874	-0.058345	4.265344
293.220936	6216.897777	15.371879	-0.058326	4.262726
293.252077	6208.861235	15.376883	-0.058327	4.260073
292.939510	6200.903200	15.381888	-0.058263	4.257441
293.121166	6192.880152	15.386893	-0.058292	4.254790
293.109753	6184.860718	15.391898	-0.058284	4.252137
293.265501	6176.852066	15.396903	-0.058308	4.249487
293.252235	6168.890734	15.401907	-0.058300	4.246850
293.021767	6160.866980	15.406912	-0.058252	4.244188
292.950637	6152.903165	15.411917	-0.058234	4.241547
293.007646	6144.901217	15.416922	-0.058239	4.238892
292.910723	6136.949074	15.421927	-0.058216	4.236250
292.649827	6128.936198	15.426931	-0.058162	4.233585
292.642863	6120.873267	15.431936	-0.058155	4.230904
292.850441	6112.914281	15.436941	-0.058189	4.228258
292.663464	6104.860195	15.441946	-0.058149	4.225575
292.685988	6096.905381	15.446951	-0.058148	4.222926
292.706978	6088.894742	15.451955	-0.058146	4.220256
292.821456	6080.903222	15.456960	-0.058162	4.217592
292.834993	6072.933775	15.461965	-0.058160	4.214932
292.741329	6064.843637	15.466970	-0.058137	4.212229
292.851421	6056.877681	15.471975	-0.058152	4.209568
292.531046	6048.904719	15.476979	-0.058087	4.206899
292.421602	6040.944440	15.481984	-0.058062	4.204234
292.426070	6032.976403	15.486989	-0.058057	4.201567
292.394000	6024.900922	15.491994	-0.058046	4.198861
292.377798	6016.932575	15.496999	-0.058038	4.196189
292.388795	6008.842856	15.502003	-0.058035	4.193476
292.194468	6000.777928	15.507008	-0.057993	4.190766
292.217478	5992.841427	15.512013	-0.057992	4.188101
292.150078	5984.845104	15.517018	-0.057974	4.185412
292.399093	5976.865973	15.522023	-0.058016	4.182732
292.056686	5968.870335	15.527027	-0.057947	4.180037
292.162305	5960.917211	15.532032	-0.057961	4.177360
292.274461	5952.900397	15.537037	-0.057977	4.174660
292.156684	5944.858411	15.542042	-0.057949	4.171947
292.246834	5936.863797	15.547047	-0.057961	4.169250
292.118597	5928.861319	15.552051	-0.057932	4.166547
292.116149	5920.900496	15.557056	-0.057926	4.163857
292.065176	5912.926162	15.562061	-0.057911	4.161161
291.923676	5904.895536	15.567066	-0.057880	4.158442
292.034147	5896.873561	15.572071	-0.057895	4.155728
291.860562	5888.862912	15.577075	-0.057857	4.153013
291.663393	5880.839064	15.582080	-0.057816	4.150291
291.680550	5872.868295	15.587085	-0.057813	4.147587
291.680798	5864.833431	15.592090	-0.057808	4.144860
291.745786	5856.894391	15.597095	-0.057815	4.142165
291.628467	5848.878809	15.602099	-0.057788	4.139439
291.560419	5840.887912	15.607104	-0.057770	4.136721
291.791988	5832.863121	15.612109	-0.057808	4.133993
291.823292	5824.825102	15.617114	-0.057808	4.131256
291.829035	5816.859277	15.622119	-0.057804	4.128542
291.492572	5808.864492	15.627123	-0.057736	4.125812
291.446012	5800.864519	15.632128	-0.057723	4.123081
291.480763	5792.897040	15.637133	-0.057724	4.120361
291.337955	5784.895718	15.642138	-0.057692	4.117626
291.528816	5776.877314	15.647143	-0.057722	4.114887
291.275037	5768.829733	15.652147	-0.057670	4.112131
291.189102	5760.806873	15.657152	-0.057648	4.109383
291.215601	5752.891760	15.662157	-0.057648	4.106672
290.997781	5744.847310	15.667162	-0.057602	4.103911
291.142908	5736.886394	15.672167	-0.057624	4.101182
291.159040	5728.886581	15.677171	-0.057622	4.098437
290.941756	5720.861160	15.682176	-0.057576	4.095677
290.888040	5712.892103	15.687181	-0.057561	4.092937
290.928344	5704.857602	15.692186	-0.057563	4.090174
290.962760	5696.865929	15.697191	-0.057564	4.087424
290.959507	5688.843052	15.702195	-0.057558	4.084661
291.110406	5680.917313	15.707200	-0.057581	4.081931
291.044332	5672.931241	15.712205	-0.057564	4.079176
290.715052	5664.897813	15.717210	-0.057497	4.076399
290.715694	5656.907366	15.722215	-0.057492	4.073639
291.031545	5648.859958	15.727219	-0.057546	4.070863
290.606927	5640.879512	15.732224	-0.057461	4.068097
290.803448	5632.898323	15.737229	-0.057493	4.065338
290.750821	5624.910141	15.742234	-0.057478	4.062571
290.648822	5616.896138	15.747239	-0.057453	4.059792
290.476788	5608.958963	15.752243	-0.057416	4.057037
290.554041	5600.921579	15.757248	-0.057425	4.054249
290.590162	5592.921972	15.762253	-0.057427	4.051472
290.465580	5584.900444	15.767258	-0.057398	4.048683
290.486837	5576.865802	15.772263	-0.057397	4.045889
290.621545	5568.940437	15.777267	-0.057417	4.043133
290.312638	5560.902132	15.782272	-0.057354	4.040330
290.366747	5552.942728	15.787277	-0.057359	4.037557
290.381980	5544.892882	15.792282	-0.057356	4.034750
290.405804	5536.806232	15.797287	-0.057355	4.031929
290.585390	5528.835591	15.802291	-0.057384	4.029149
290.460135	5520.841645	15.807296	-0.057355	4.026354
290.468410	5512.901037	15.812301	-0.057351	4.023577
290.301593	5504.887961	15.817306	-0.057315	4.020771
290.258406	5496.934833	15.822311	-0.057302	4.017985
290.244041	5488.890667	15.827315	-0.057294	4.015166
290.190786	5480.842320	15.832320	-0.057279	4.012344
290.298545	5472.846742	15.837325	-0.057293	4.009540
290.170817	5464.908150	15.842330	-0.057264	4.006750
290.116068	5456.905252	15.847335	-0.057249	4.003937
289.968515	5448.927288	15.852339	-0.057216	4.001130
289.944307	5440.918354	15.857344	-0.057207	3.998311
290.012065	5432.884307	15.862349	-0.057214	3.995483
289.814946	5424.860960	15.867354	-0.057172	3.992653
289.836658	5416.853693	15.872359	-0.057171	3.989830
290.108025	5408.873297	15.877363	-0.057216	3.987018
289.980451	5400.868300	15.882368	-0.057187	3.984189
289.882075	5392.941876	15.887373	-0.057163	3.981386
289.736701	5384.895309	15.892378	-0.057131	3.978539
289.740473	5376.901371	15.897383	-0.057127	3.975710
289.629723	5368.902661	15.902387	-0.057101	3.972875
289.645576	5360.840318	15.907392	-0.057098	3.970018
289.770629	5352.918514	15.912397	-0.057116	3.967211
289.546390	5344.896694	15.917402	-0.057069	3.964360
289.313378	5336.963769	15.922407	-0.057021	3.961539
289.627547	5328.954973	15.927411	-0.057074	3.958698
289.405198	5320.946985	15.932416	-0.057027	3.955846
289.501555	5312.938197	15.937421	-0.057040	3.952997
289.532246	5304.865619	15.942426	-0.057041	3.950122
289.387384	5296.919560	15.947431	-0.057008	3.947288
289.356191	5288.922957	15.952435	-0.056997	3.944435
289.344977	5280.959153	15.957440	-0.056990	3.941592
289.338323	5272.942345	15.962445	-0.056983	3.938728
289.132354	5264.970078	15.967450	-0.056940	3.935874
289.105485	5256.972955	15.972455	-0.056930	3.933013
289.356550	5248.917208	15.977459	-0.056971	3.930134
289.204867	5240.958917	15.982464	-0.056938	3.927280
289.228140	5232.969809	15.987469	-0.056937	3.924416
289.071083	5224.982606	15.992474	-0.056902	3.921548
288.992807	5216.979935	15.997479	-0.056882	3.918673
288.956510	5208.981905	16.002483	-0.056870	3.915798
288.874987	5200.926122	16.007488	-0.056850	3.912900
289.066484	5192.928239	16.012493	-0.056880	3.910026
288.829189	5184.946138	16.017498	-0.056831	3.907147
288.875520	5176.956216	16.022503	-0.056834	3.904269
288.832448	5168.977682	16.027507	-0.056821	3.901390
288.887813	5160.966205	16.032512	-0.056826	3.898500
288.886133	5152.995609	16.037517	-0.056820	3.895621
288.783424	5144.930016	16.042522	-0.056796	3.892704
288.752517	5136.903835	16.047527	-0.056785	3.889800
288.662028	5128.992002	16.052531	-0.056763	3.886935
288.381438	5120.977257	16.057536	-0.056705	3.884026
288.731298	5112.966029	16.062541	-0.056765	3.881128
288.702192	5104.956829	16.067546	-0.056755	3.878222
288.583020	5096.976538	16.072551	-0.056727	3.875322
288.345880	5088.800777	16.077555	-0.056678	3.872347
288.369520	5080.766642	16.082560	-0.056677	3.869426
288.315094	5072.873164	16.087565	-0.056662	3.866553
288.120184	5064.877544	16.092570	-0.056620	3.863637
288.338876	5056.916822	16.097575	-0.056655	3.860740
288.350365	5048.956241	16.102579	-0.056652	3.857837
288.332541	5040.927169	16.107584	-0.056644	3.854906
288.419695	5032.972751	16.112589	-0.056655	3.852002
288.400737	5024.931149	16.117594	-0.056646	3.849062
288.204026	5016.985783	16.122599	-0.056604	3.846152
288.168434	5009.003432	16.127603	-0.056592	3.843228
288.183053	5000.979219	16.132608	-0.056590	3.840289
288.154653	4993.052937	16.137613	-0.056579	3.837382
288.008442	4985.005800	16.142618	-0.056547	3.834426
288.202785	4976.988156	16.147623	-0.056578	3.831486
287.932869	4968.977477	16.152627	-0.056522	3.828536
287.699640	4960.971854	16.157632	-0.056473	3.825587
287.820553	4953.035353	16.162637	-0.056491	3.822668
287.884856	4945.000522	16.167642	-0.056497	3.819709
287.805662	4937.080047	16.172647	-0.056478	3.816788
287.848604	4929.040198	16.177651	-0.056480	3.813823
287.626082	4921.014365	16.182656	-0.056434	3.810854
287.696016	4913.054741	16.187661	-0.056441	3.807915
287.696264	4904.997284	16.192666	-0.056436	3.804935
287.803674	4897.071421	16.197671	-0.056451	3.802004
287.794250	4889.075072	16.202675	-0.056444	3.799042
287.397564	4881.093472	16.207680	-0.056365	3.796075
287.479070	4873.038708	16.212685	-0.056375	3.793089
287.420115	4865.009516	16.217690	-0.056358	3.790107
287.417318	4857.021133	16.222695	-0.056353	3.787139
287.420287	4849.047069	16.227699	-0.056348	3.784174
287.400249	4841.052124	16.232704	-0.056339	3.781198
287.425508	4833.071660	16.237709	-0.056338	3.778227
287.144410	4825.067369	16.242714	-0.056281	3.775237
287.128116	4817.065250	16.247719	-0.056273	3.772252
287.346006	4809.041900	16.252723	-0.056308	3.769262
287.268980	4801.041103	16.257728	-0.056288	3.766271
287.218406	4793.080141	16.262733	-0.056274	3.763293
287.176143	4785.064954	16.267738	-0.056260	3.760293
287.196529	4777.084839	16.272743	-0.056259	3.757305
287.046509	4769.078273	16.277747	-0.056226	3.754300
287.020795	4761.028073	16.282752	-0.056216	3.751280
286.983604	4753.060734	16.287757	-0.056204	3.748288
287.030538	4745.033079	16.292762	-0.056207	3.745273
287.088150	4737.090886	16.297767	-0.056213	3.742288
287.243422	4729.090846	16.302771	-0.056236	3.739282
287.063574	4721.073473	16.307776	-0.056198	3.736258
287.002340	4713.111506	16.312781	-0.056181	3.733256
286.882534	4705.050475	16.317786	-0.056153	3.730212
286.652626	4697.106386	16.322791	-0.056105	3.727207
286.873278	4689.117047	16.327795	-0.056141	3.724194
286.851466	4681.119831	16.332800	-0.056132	3.721169
286.723167	4673.172225	16.337805	-0.056103	3.718158
286.580226	4665.148840	16.342810	-0.056071	3.715116
286.574940	4657.048325	16.347815	-0.056065	3.712045
286.544932	4649.057294	16.352819	-0.056054	3.709013
286.306124	4641.110988	16.357824	-0.056004	3.705990
286.586348	4633.144977	16.362829	-0.056051	3.702970
286.700531	4625.125590	16.367834	-0.056067	3.699923
286.541960	4617.174029	16.372839	-0.056032	3.696892
286.353201	4609.194996	16.377843	-0.055992	3.693848
286.231011	4601.141317	16.382848	-0.055964	3.690774
286.382233	4593.160633	16.387853	-0.055987	3.687733
286.072456	4585.161363	16.392858	-0.055924	3.684670
286.118847	4577.206523	16.397863	-0.055927	3.681631
286.183422	4569.228475	16.402867	-0.055934	3.678581
286.152125	4561.194126	16.407872	-0.055923	3.675504
286.065589	4553.171031	16.412877	-0.055901	3.672427
285.939501	4545.160611	16.417882	-0.055873	3.669352
286.052811	4537.173395	16.422887	-0.055889	3.666290
286.222284	4529.202834	16.427891	-0.055915	3.663232
286.132940	4521.173564	16.432896	-0.055893	3.660143
286.154632	4513.231991	16.437901	-0.055892	3.657088
285.908231	4505.224524	16.442906	-0.055841	3.653998
285.844147	4497.193699	16.447911	-0.055823	3.650901
286.097123	4489.228128	16.452915	-0.055865	3.647834
285.763375	4481.191378	16.457920	-0.055798	3.644723
285.842187	4473.262486	16.462925	-0.055807	3.641661
285.764814	4465.241265	16.467930	-0.055788	3.638557
285.772076	4457.260581	16.472935	-0.055784	3.635468
285.755398	4449.233566	16.477939	-0.055775	3.632358
285.581367	4441.178509	16.482944	-0.055738	3.629230
285.701306	4433.228186	16.487949	-0.055755	3.626148
285.589576	4425.232483	16.492954	-0.055729	3.623039
285.546883	4417.235646	16.497959	-0.055716	3.619929
285.605361	4409.277892	16.502963	-0.055721	3.616835
285.537396	4401.233268	16.507968	-0.055703	3.613700
285.583220	4393.253270	16.512973	-0.055707	3.610591
285.653221	4385.252016	16.517978	-0.055714	3.607472
285.424048	4377.254949	16.522983	-0.055666	3.604344
285.608841	4369.331256	16.527987	-0.055696	3.601253
285.453975	4361.346807	16.532992	-0.055662	3.598126
285.525702	4353.338783	16.537997	-0.055670	3.594993
285.231802	4345.339298	16.543002	-0.055610	3.591851
285.311228	4337.287418	16.548007	-0.055619	3.588696
285.299616	4329.317550	16.553011	-0.055612	3.585567
285.117107	4321.341607	16.558016	-0.055573	3.582429
285.232573	4313.344745	16.563021	-0.055589	3.579288
284.994082	4305.390154	16.568026	-0.055539	3.576151
284.992634	4297.353242	16.573031	-0.055534	3.572986
285.172097	4289.335543	16.578035	-0.055562	3.569831
285.132295	4281.358356	16.583040	-0.055549	3.566682
285.088715	4273.360067	16.588045	-0.055536	3.563522
285.035356	4265.379094	16.593050	-0.055521	3.560366
285.022743	4257.410889	16.598055	-0.055513	3.557214
285.171421	4249.363708	16.603059	-0.055535	3.554032
284.997471	4241.277592	16.608064	-0.055498	3.550822
284.858438	4233.350462	16.613069	-0.055467	3.547673
284.780032	4225.332370	16.618074	-0.055447	3.544488
284.897394	4217.377528	16.623079	-0.055463	3.541330
285.026966	4209.399786	16.628083	-0.055482	3.538161
284.706574	4201.401901	16.633088	-0.055417	3.534967
284.723399	4193.406282	16.638093	-0.055415	3.531782
284.658888	4185.377869	16.643098	-0.055398	3.528578
284.666136	4177.378695	16.648103	-0.055394	3.525385
284.700350	4169.444858	16.653107	-0.055395	3.522217
284.557080	4161.433373	16.658112	-0.055363	3.519008
284.568757	4153.471203	16.663117	-0.055360	3.515822
284.321105	4145.439560	16.668122	-0.055309	3.512596
284.361794	4137.407245	16.673127	-0.055311	3.509377
284.440623	4129.450878	16.678131	-0.055321	3.506186
284.288857	4121.479152	16.683136	-0.055287	3.502978
284.305217	4113.481598	16.688141	-0.055285	3.499763
284.390274	4105.512418	16.693146	-0.055296	3.496558
284.139371	4097.526319	16.698151	-0.055244	3.493333
284.163460	4089.483685	16.703155	-0.055243	3.490091
284.124751	4081.493638	16.708160	-0.055230	3.486865
284.140391	4073.544597	16.713165	-0.055228	3.483655
284.036340	4065.540520	16.718170	-0.055203	3.480415
284.058033	4057.561024	16.723175	-0.055202	3.477186
283.934684	4049.554176	16.728179	-0.055174	3.473939
283.646935	4041.518649	16.733184	-0.055115	3.470671
283.791363	4033.525703	16.738189	-0.055137	3.467432
283.742258	4025.541746	16.743194	-0.055122	3.464187
283.694077	4017.540666	16.748199	-0.055108	3.460932
283.776839	4009.591102	16.753203	-0.055118	3.457699
283.747239	4001.566032	16.758208	-0.055108	3.454429
283.919574	3993.563724	16.763213	-0.055134	3.451171
283.810917	3985.565543	16.768218	-0.055109	3.447903
283.910560	3977.553594	16.773223	-0.055122	3.444633
283.678649	3969.665336	16.778227	-0.055074	3.441399
283.381180	3961.637451	16.783232	-0.055013	3.438104
283.526781	3953.646104	16.788237	-0.055035	3.434834
283.404231	3945.620252	16.793242	-0.055007	3.431539
283.418133	3937.621426	16.798247	-0.055004	3.428256
283.347732	3929.599197	16.803251	-0.054986	3.424957
283.387029	3921.650078	16.808256	-0.054988	3.421689
283.331904	3913.657190	16.813261	-0.054973	3.418396
283.343007	3905.671870	16.818266	-0.054969	3.415106
283.221947	3897.669620	16.823271	-0.054942	3.411801
283.258634	3889.680247	16.828275	-0.054943	3.408504
283.187385	3881.675850	16.833280	-0.054925	3.405193
283.381814	3873.723529	16.838285	-0.054956	3.401910
283.245820	3865.728761	16.843290	-0.054925	3.398595
283.119674	3857.735016	16.848295	-0.054896	3.395277
283.056742	3849.682176	16.853299	-0.054879	3.391934
283.001620	3841.650929	16.858304	-0.054864	3.388596
283.058458	3833.682745	16.863309	-0.054869	3.385286
282.906501	3825.742964	16.868314	-0.054836	3.381976
283.092968	3817.752423	16.873319	-0.054865	3.378654
282.995274	3809.766071	16.878323	-0.054842	3.375321
282.884176	3801.754406	16.883328	-0.054816	3.371973
282.955322	3793.747923	16.888333	-0.054824	3.368631
282.842302	3785.783741	16.893338	-0.054797	3.365296
282.633482	3777.832728	16.898343	-0.054753	3.361960
282.650286	3769.842800	16.903347	-0.054751	3.358613
282.728631	3761.815370	16.908352	-0.054761	3.355249
282.775257	3753.815786	16.913357	-0.054764	3.351892
282.721021	3745.800985	16.918362	-0.054749	3.348521
282.490864	3737.793195	16.923367	-0.054700	3.345144
282.499560	3729.874394	16.928371	-0.054697	3.341809
282.553336	3721.838183	16.933376	-0.054702	3.338423
282.752651	3713.859535	16.938381	-0.054733	3.335064
282.636695	3705.873527	16.943386	-0.054707	3.331686
282.593590	3697.874541	16.948391	-0.054693	3.328302
282.429855	3689.909041	16.953395	-0.054658	3.324924
282.343711	3681.930903	16.958400	-0.054636	3.321541
282.380177	3673.944987	16.963405	-0.054638	3.318155
282.197038	3665.946915	16.968410	-0.054599	3.314752
282.234023	3657.902425	16.973415	-0.054600	3.311335
282.254352	3649.908776	16.978419	-0.054599	3.307934
281.974329	3641.903880	16.983424	-0.054541	3.304515
282.099141	3633.954052	16.988429	-0.054559	3.301130
281.996631	3625.966080	16.993434	-0.054535	3.297717
282.027928	3617.959852	16.998439	-0.054536	3.294298
282.073723	3609.995648	17.003443	-0.054539	3.290894
281.763622	3602.006774	17.008448	-0.054476	3.287462
281.976878	3594.004754	17.013453	-0.054510	3.284041
282.093201	3586.024814	17.018458	-0.054527	3.280622
282.060012	3578.059395	17.023463	-0.054515	3.277200
282.119094	3570.048951	17.028467	-0.054521	3.273758
282.076932	3562.012597	17.033472	-0.054508	3.270298
282.044980	3554.060619	17.038477	-0.054497	3.266871
281.975548	3546.090758	17.043482	-0.054479	3.263431
281.882957	3538.090979	17.048487	-0.054456	3.259974
281.647501	3530.130147	17.053491	-0.054407	3.256524
281.537754	3522.099257	17.058496	-0.054381	3.253045
281.664671	3514.094152	17.063501	-0.054400	3.249583
281.619298	3506.129233	17.068506	-0.054386	3.246128
281.536656	3498.161165	17.073511	-0.054365	3.242667
281.616333	3490.172263	17.078515	-0.054375	3.239199
281.473698	3482.188827	17.083520	-0.054343	3.235720
281.545773	3474.133898	17.088525	-0.054351	3.232216
281.318727	3466.150608	17.093530	-0.054304	3.228727
281.360827	3458.126631	17.098535	-0.054306	3.225227
281.534843	3450.183294	17.103539	-0.054334	3.221764
281.349178	3442.210774	17.108544	-0.054294	3.218270
281.439053	3434.212578	17.113549	-0.054305	3.214772
281.264238	3426.231579	17.118554	-0.054268	3.211267
281.129136	3418.244259	17.123559	-0.054237	3.207757
281.308224	3410.236065	17.128563	-0.054265	3.204247
281.138753	3402.270274	17.133568	-0.054228	3.200737
281.159278	3394.295280	17.138573	-0.054227	3.197227
281.056118	3386.306101	17.143578	-0.054203	3.193702
281.055750	3378.274984	17.148583	-0.054197	3.190159
281.119174	3370.289092	17.153587	-0.054204	3.186635
281.112532	3362.313768	17.158592	-0.054197	3.183108
280.972565	3354.361478	17.163597	-0.054166	3.179582
280.796485	3346.397608	17.168602	-0.054128	3.176045
280.652143	3338.370719	17.173607	-0.054096	3.172478
280.775651	3330.366449	17.178611	-0.054114	3.168929
280.675833	3322.373017	17.183616	-0.054090	3.165370
280.663185	3314.422245	17.188621	-0.054082	3.161830
280.747157	3306.433905	17.193626	-0.054093	3.158274
280.967970	3298.390869	17.198631	-0.054128	3.154695
280.850891	3290.411415	17.203635	-0.054101	3.151126
280.526979	3282.431239	17.208640	-0.054036	3.147544
280.674914	3274.431606	17.213645	-0.054058	3.143969
280.469203	3266.490265	17.218650	-0.054015	3.140401
280.486164	3258.500732	17.223655	-0.054012	3.136817
280.391241	3250.508406	17.228659	-0.053990	3.133223
280.166847	3242.486025	17.233664	-0.053943	3.129605
280.207959	3234.527209	17.238669	-0.053945	3.126023
280.332145	3226.546436	17.243674	-0.053963	3.122431
280.229097	3218.562739	17.248679	-0.053938	3.118824
280.256339	3210.622357	17.253683	-0.053938	3.115238
280.020259	3202.600041	17.258688	-0.053889	3.111598
280.255760	3194.597402	17.263693	-0.053928	3.107985
280.369537	3186.574134	17.268698	-0.053944	3.104352
280.073291	3178.645921	17.273703	-0.053883	3.100740
280.020994	3170.668305	17.278707	-0.053868	3.097112
280.095579	3162.629711	17.283712	-0.053877	3.093458
279.980833	3154.657313	17.288717	-0.053850	3.089822
280.013696	3146.675369	17.293722	-0.053851	3.086183
279.890376	3138.689907	17.298727	-0.053823	3.082531
279.937656	3130.735605	17.303731	-0.053826	3.078897
279.792139	3122.752282	17.308736	-0.053794	3.075237
279.881283	3114.663449	17.313741	-0.053805	3.071534
279.632819	3106.691473	17.318746	-0.053754	3.067865
279.547996	3098.702959	17.323751	-0.053733	3.064192
279.774803	3090.736317	17.328755	-0.053770	3.060539
279.740551	3082.760404	17.333760	-0.053758	3.056865
279.630024	3074.795158	17.338765	-0.053732	3.053188
279.534158	3066.795470	17.343770	-0.053709	3.049491
279.447969	3058.822767	17.348775	-0.053688	3.045803
279.702622	3050.849553	17.353779	-0.053730	3.042126
279.438499	3042.882897	17.358784	-0.053676	3.038423
279.495498	3034.891489	17.363789	-0.053681	3.034719
279.454384	3026.892440	17.368794	-0.053668	3.031003
279.131378	3018.915080	17.373799	-0.053603	3.027278
279.214104	3010.930921	17.378803	-0.053613	3.023566
279.183309	3002.947621	17.383808	-0.053602	3.019843
279.332771	2994.983421	17.388813	-0.053625	3.016134
279.058851	2986.979124	17.393818	-0.053568	3.012381
279.298172	2978.947772	17.398823	-0.053608	3.008635
279.361692	2970.986744	17.403827	-0.053614	3.004909
279.121718	2963.044231	17.408832	-0.053564	3.001173
279.168108	2955.082191	17.413837	-0.053568	2.997436
279.162990	2947.075774	17.418842	-0.053562	2.993672
278.977104	2939.046876	17.423847	-0.053522	2.989883
278.948005	2931.102970	17.428851	-0.053511	2.986137
278.939792	2923.090140	17.433856	-0.053504	2.982355
278.786080	2915.135323	17.438861	-0.053470	2.978588
278.670930	2907.166094	17.443866	-0.053444	2.974812
278.604949	2899.145814	17.448871	-0.053426	2.971009
278.739467	2891.162392	17.453875	-0.053446	2.967229
278.697548	2883.168581	17.458880	-0.053433	2.963430
278.509003	2875.225724	17.463885	-0.053393	2.959643
278.673068	2867.258463	17.468890	-0.053418	2.955858
278.440198	2859.240072	17.473895	-0.053369	2.952023
278.477770	2851.259872	17.478899	-0.053371	2.948215
278.495821	2843.258136	17.483904	-0.053369	2.944391
278.464386	2835.322995	17.488909	-0.053358	2.940591
278.292422	2827.365864	17.493914	-0.053321	2.936768
278.136304	2819.349849	17.498919	-0.053287	2.932913
278.462758	2811.311998	17.503923	-0.053342	2.929068
278.379250	2803.344197	17.508928	-0.053321	2.925230
278.266496	2795.431542	17.513933	-0.053295	2.921411
278.387694	2787.428643	17.518938	-0.053312	2.917557
278.131662	2779.440840	17.523943	-0.053260	2.913685
277.999842	2771.391443	17.528947	-0.053230	2.909784
278.173241	2763.392084	17.533952	-0.053257	2.905919
278.154054	2755.445752	17.538957	-0.053248	2.902064
278.279292	2747.456125	17.543962	-0.053266	2.898190
277.994147	2739.507790	17.548967	-0.053208	2.894310
278.070426	2731.516732	17.553971	-0.053217	2.890422
277.841941	2723.540168	17.558976	-0.053169	2.886521
277.780502	2715.584676	17.563981	-0.053152	2.882633
277.812709	2707.610368	17.568986	-0.053153	2.878736
277.487798	2699.653585	17.573991	-0.053087	2.874822
277.526754	2691.644837	17.578995	-0.053089	2.870898
277.376314	2683.660615	17.584000	-0.053056	2.866970
277.629359	2675.660530	17.589005	-0.053098	2.863051
277.522854	2667.683807	17.594010	-0.053073	2.859118
277.581913	2659.695039	17.599015	-0.053079	2.855183
277.584609	2651.709075	17.604019	-0.053074	2.851241
277.425594	2643.757481	17.609024	-0.053039	2.847301
277.287129	2635.802676	17.614029	-0.053008	2.843355
277.466743	2627.816623	17.619034	-0.053036	2.839407
277.360198	2619.851463	17.624039	-0.053011	2.835447
277.140475	2611.878987	17.629043	-0.052965	2.831471
277.005866	2603.863003	17.634048	-0.052935	2.827473
277.058516	2595.863959	17.639053	-0.052939	2.823489
276.976699	2587.907181	17.644058	-0.052919	2.819512
276.928995	2579.934675	17.649063	-0.052905	2.815523
277.151890	2571.925612	17.654067	-0.052941	2.811527
276.887842	2563.952676	17.659072	-0.052886	2.807514
276.737236	2556.001211	17.664077	-0.052853	2.803513
276.923379	2548.028545	17.669082	-0.052883	2.799516
276.793893	2540.068311	17.674087	-0.052853	2.795500
276.792862	2532.076877	17.679091	-0.052848	2.791471
276.747116	2524.068803	17.684096	-0.052834	2.787424
276.839277	2516.083515	17.689101	-0.052846	2.783391
276.752277	2508.133048	17.694106	-0.052825	2.779360
276.576575	2500.188504	17.699111	-0.052787	2.775320
276.648101	2492.192991	17.704115	-0.052795	2.771264
276.765837	2484.161425	17.709120	-0.052811	2.767185
276.487839	2476.251654	17.714125	-0.052754	2.763140
276.593175	2468.259748	17.719130	-0.052769	2.759069
276.574075	2460.296024	17.724135	-0.052760	2.754999
276.408270	2452.255857	17.729139	-0.052724	2.750875
276.331597	2444.273952	17.734144	-0.052704	2.746780
276.440535	2436.285731	17.739149	-0.052719	2.742687
276.426648	2428.337246	17.744154	-0.052712	2.738601
276.417308	2420.361909	17.749159	-0.052705	2.734496
276.474652	2412.383987	17.754163	-0.052710	2.730386
276.405029	2404.416207	17.759168	-0.052692	2.726269
276.259710	2396.458651	17.764173	-0.052660	2.722145
276.280948	2388.512056	17.769178	-0.052658	2.718031
276.239959	2380.522350	17.774183	-0.052645	2.713885
276.264162	2372.529273	17.779187	-0.052645	2.709734
275.937726	2364.574232	17.784192	-0.052579	2.705576
276.050007	2356.596340	17.789197	-0.052594	2.701426
276.142408	2348.617486	17.794202	-0.052606	2.697268
276.061343	2340.632959	17.799207	-0.052586	2.693090
275.992792	2332.665914	17.804211	-0.052568	2.688915
275.914561	2324.695192	17.809216	-0.052548	2.684731
275.723780	2316.777282	17.814221	-0.052507	2.680561
275.765103	2308.795640	17.819226	-0.052510	2.676366
275.830024	2300.763807	17.824231	-0.052517	2.672140
275.631601	2292.806205	17.829235	-0.052474	2.667929
275.436766	2284.818925	17.834240	-0.052433	2.663696
275.596975	2276.838310	17.839245	-0.052458	2.659482
275.852777	2268.866226	17.844250	-0.052500	2.655273
275.529813	2260.899259	17.849255	-0.052435	2.651022
275.631640	2252.936933	17.854259	-0.052448	2.646794
275.806942	2244.932865	17.859264	-0.052476	2.642542
275.695771	2237.009221	17.864269	-0.052450	2.638308
275.474507	2229.065495	17.869274	-0.052403	2.634049
275.428301	2221.039442	17.874279	-0.052390	2.629750
275.440373	2213.091787	17.879283	-0.052387	2.625490
275.366134	2205.118021	17.884288	-0.052367	2.621203
275.276416	2197.173175	17.889293	-0.052346	2.616924
275.330849	2189.195993	17.894298	-0.052350	2.612630
275.210375	2181.198408	17.899303	-0.052323	2.608306
275.151377	2173.249212	17.904307	-0.052307	2.604005
275.151361	2165.274717	17.909312	-0.052301	2.599688
275.062888	2157.340898	17.914317	-0.052280	2.595379
274.986877	2149.192212	17.919322	-0.052260	2.590947
275.136885	2141.191733	17.924327	-0.052283	2.586604
275.052783	2133.281446	17.929331	-0.052262	2.582287
274.966570	2125.360704	17.934336	-0.052241	2.577956
275.060114	2117.384514	17.939341	-0.052253	2.573600
274.983868	2109.422938	17.944346	-0.052233	2.569233
274.792538	2101.467285	17.949351	-0.052193	2.564854
274.803415	2093.539224	17.954355	-0.052189	2.560497
274.650081	2085.573479	17.959360	-0.052156	2.556100
274.552596	2077.602294	17.964365	-0.052132	2.551696
274.654765	2069.594466	17.969370	-0.052146	2.547278
274.453075	2061.657114	17.974375	-0.052103	2.542871
274.542042	2053.708740	17.979379	-0.052115	2.538470
274.336990	2045.743901	17.984384	-0.052071	2.534031
274.560465	2037.726373	17.989389	-0.052108	2.529586
274.419526	2029.789818	17.994394	-0.052076	2.525152
274.175160	2021.844775	17.999399	-0.052025	2.520698
274.420000	2013.883242	18.004403	-0.052066	2.516262
274.467185	2005.873866	18.009408	-0.052069	2.511778
274.402634	1997.894243	18.014413	-0.052052	2.507294
274.221790	1989.966651	18.019418	-0.052013	2.502822
274.036380	1982.011289	18.024423	-0.051973	2.498327
274.022143	1974.057631	18.029427	-0.051966	2.493837
274.021324	1966.050640	18.034432	-0.051960	2.489309
273.969109	1958.102040	18.039437	-0.051945	2.484803
274.003879	1950.166215	18.044442	-0.051946	2.480302
274.046351	1942.185882	18.049447	-0.051949	2.475769
274.014047	1934.214808	18.054451	-0.051938	2.471226
273.772840	1926.265138	18.059456	-0.051888	2.466672
273.718401	1918.315730	18.064461	-0.051872	2.462124
273.713647	1910.354936	18.069466	-0.051866	2.457564
273.843809	1902.358630	18.074471	-0.051885	2.452986
273.690642	1894.405095	18.079475	-0.051851	2.448402
273.462803	1886.461187	18.084480	-0.051804	2.443809
273.552129	1878.507390	18.089485	-0.051815	2.439227
273.505794	1870.570429	18.094490	-0.051801	2.434635
273.498535	1862.494686	18.099495	-0.051795	2.429956
273.387089	1854.567300	18.104499	-0.051769	2.425347
273.439808	1846.600874	18.109504	-0.051773	2.420719
273.489201	1838.649278	18.114509	-0.051777	2.416091
273.291430	1830.699983	18.119514	-0.051735	2.411436
273.368406	1822.719250	18.124519	-0.051744	2.406775
273.411757	1814.779686	18.129523	-0.051747	2.402126
273.231361	1806.843831	18.134528	-0.051708	2.397453
273.194138	1798.893315	18.139533	-0.051696	2.392774
273.257417	1790.896250	18.144538	-0.051703	2.388065
273.099453	1782.951118	18.149543	-0.051668	2.383361
273.411766	1774.986412	18.154547	-0.051721	2.378673
273.157240	1767.054616	18.159552	-0.051669	2.373950
273.007596	1759.105239	18.164557	-0.051635	2.369216
273.040578	1751.141757	18.169562	-0.051636	2.364478
272.713409	1743.231246	18.174567	-0.051570	2.359734
272.870520	1735.259476	18.179571	-0.051594	2.354982
272.792090	1727.248290	18.184576	-0.051574	2.350178
272.830562	1719.273041	18.189581	-0.051576	2.345395
273.023878	1711.316633	18.194586	-0.051607	2.340627
272.814728	1703.400140	18.199591	-0.051563	2.335840
272.644863	1695.456954	18.204595	-0.051526	2.331030
272.482648	1687.506286	18.209600	-0.051491	2.326206
272.691105	1679.528104	18.214605	-0.051524	2.321386
272.512597	1671.621737	18.219610	-0.051486	2.316568
272.420412	1663.633042	18.224615	-0.051463	2.311696
272.570935	1655.665070	18.229619	-0.051486	2.306847
272.390136	1647.724729	18.234624	-0.051447	2.301978
272.380053	1639.789316	18.239629	-0.051440	2.297115
272.307471	1631.829008	18.244634	-0.051422	2.292221
272.065429	1623.878404	18.249639	-0.051371	2.287308
272.233644	1615.930450	18.254643	-0.051397	2.282422
272.338908	1607.974016	18.259648	-0.051412	2.277514
272.265274	1599.992406	18.264653	-0.051393	2.272565
271.983023	1592.032732	18.269658	-0.051335	2.267600
272.110495	1584.056430	18.274663	-0.051353	2.262650
272.176528	1576.125774	18.279667	-0.051361	2.257712
271.937852	1568.201857	18.284672	-0.051311	2.252740
271.998757	1560.224243	18.289677	-0.051317	2.247751
272.069639	1552.285756	18.294682	-0.051325	2.242775
271.772591	1544.377259	18.299687	-0.051265	2.237775
271.543299	1536.459100	18.304691	-0.051217	2.232764
271.496851	1528.472060	18.309696	-0.051203	2.227714
271.486322	1520.522247	18.314701	-0.051196	2.222679
271.578965	1512.586276	18.319706	-0.051208	2.217651
271.588394	1504.615450	18.324711	-0.051204	2.212582
271.480701	1496.686201	18.329715	-0.051179	2.207517
271.524860	1488.732825	18.334720	-0.051182	2.202439
271.506445	1480.805359	18.339725	-0.051173	2.197360
271.418566	1472.858918	18.344730	-0.051152	2.192251
271.254331	1464.894362	18.349735	-0.051116	2.187111
271.226836	1456.971316	18.354739	-0.051106	2.181998
271.009144	1449.047286	18.359744	-0.051060	2.176855
271.065509	1441.072143	18.364749	-0.051065	2.171692
271.100115	1433.131006	18.369754	-0.051066	2.166537
271.067067	1425.185322	18.374759	-0.051055	2.161360
271.037893	1417.270550	18.379763	-0.051044	2.156192
271.044375	1409.288167	18.384768	-0.051040	2.150970
270.900230	1401.361908	18.389773	-0.051008	2.145758
270.935433	1393.444718	18.394778	-0.051010	2.140556
270.836803	1385.516247	18.399783	-0.050986	2.135321
270.727086	1377.574175	18.404787	-0.050960	2.130063
270.737133	1369.621132	18.409792	-0.050957	2.124797
270.729799	1361.694040	18.414797	-0.050950	2.119533
270.677132	1353.777237	18.419802	-0.050935	2.114258
270.413769	1345.773022	18.424807	-0.050881	2.108892
270.397798	1337.850999	18.429811	-0.050873	2.103590
270.549670	1329.901625	18.434816	-0.050896	2.098274
270.427589	1321.973954	18.439821	-0.050868	2.092931
270.313534	1314.058725	18.444826	-0.050842	2.087584
270.106476	1306.143219	18.449831	-0.050798	2.082214
270.441634	1298.193047	18.454835	-0.050855	2.076860
270.183371	1290.266283	18.459840	-0.050802	2.071450
270.265339	1282.304117	18.464845	-0.050812	2.066035
270.257841	1274.386314	18.469850	-0.050805	2.060627
270.076367	1266.474209	18.474855	-0.050766	2.055191
270.058952	1258.545493	18.479859	-0.050758	2.049746
270.101385	1250.598482	18.484864	-0.050760	2.044280
270.000504	1242.706822	18.489869	-0.050736	2.038823
270.009089	1234.774968	18.494874	-0.050733	2.033334
269.841747	1226.829530	18.499879	-0.050696	2.027803
269.935708	1218.898708	18.504883	-0.050709	2.022294
269.772975	1210.991329	18.509888	-0.050673	2.016760
269.988191	1203.013117	18.514893	-0.050708	2.011201
269.882184	1195.111433	18.519898	-0.050683	2.005646
269.531923	1187.241537	18.524903	-0.050613	2.000072
269.518624	1179.334538	18.529907	-0.050605	1.994492
269.637878	1171.347991	18.534912	-0.050622	1.988854
269.549307	1163.434665	18.539917	-0.050600	1.983230
269.397002	1155.549602	18.544922	-0.050567	1.977604
269.320529	1147.607823	18.549927	-0.050547	1.971929
269.410075	1139.673508	18.554931	-0.050559	1.966260
269.217366	1131.790071	18.559936	-0.050518	1.960582
269.199428	1123.875926	18.564941	-0.050509	1.954883
269.164639	1115.911149	18.569946	-0.050498	1.949130
268.995707	1107.985938	18.574951	-0.050461	1.943373
269.098408	1100.073318	18.579955	-0.050475	1.937638
268.968800	1092.155416	18.584960	-0.050446	1.931857
269.032214	1084.217266	18.589965	-0.050452	1.926065
268.894049	1076.341413	18.594970	-0.050421	1.920279
269.033826	1068.404757	18.599975	-0.050442	1.914461
269.064982	1060.476161	18.604979	-0.050443	1.908620
268.962966	1052.564339	18.609984	-0.050418	1.902758
268.755835	1044.699618	18.614989	-0.050375	1.896901
268.900567	1036.761694	18.619994	-0.050396	1.891011
268.541657	1028.885458	18.624999	-0.050324	1.885092
268.593808	1020.991426	18.630003	-0.050329	1.879187
268.502952	1013.079597	18.635008	-0.050307	1.873235
268.506363	1005.136584	18.640013	-0.050302	1.867250
268.392343	997.248487	18.645018	-0.050276	1.861274
268.250984	989.357292	18.650023	-0.050244	1.855274
268.403931	981.422658	18.655027	-0.050268	1.849255
268.297465	973.532241	18.660032	-0.050243	1.843220
268.341651	965.638479	18.665037	-0.050246	1.837180
268.302855	957.725753	18.670042	-0.050233	1.831096
268.184854	949.822404	18.675047	-0.050206	1.824989
268.005284	941.972594	18.680051	-0.050167	1.818896
267.996094	934.066684	18.685056	-0.050161	1.812759
268.122951	926.123663	18.690061	-0.050179	1.806589
268.057031	918.265567	18.695066	-0.050162	1.800441
267.893519	910.378894	18.700071	-0.050126	1.794237
268.063535	902.402905	18.705075	-0.050152	1.787982
267.706545	894.561731	18.710080	-0.050081	1.781748
267.679809	886.676286	18.715085	-0.050071	1.775496
267.787202	878.755378	18.720090	-0.050085	1.769211
267.490112	870.911262	18.725095	-0.050025	1.762915
267.493537	863.038967	18.730099	-0.050020	1.756611
267.419157	855.127937	18.735104	-0.050001	1.750244
267.602614	847.211755	18.740109	-0.050030	1.743881
267.662959	839.341982	18.745114	-0.050036	1.737517
267.327999	831.486611	18.750119	-0.049969	1.731092
267.442479	823.599087	18.755123	-0.049985	1.724673
267.353984	815.746598	18.760128	-0.049963	1.718233
267.239036	807.861762	18.765133	-0.049937	1.711739
267.308054	799.954117	18.770138	-0.049944	1.705225
267.072372	792.117678	18.775143	-0.049895	1.698705
267.142051	784.223527	18.780147	-0.049903	1.692153
267.012639	776.354350	18.785152	-0.049874	1.685569
266.915468	768.510511	18.790157	-0.049851	1.678985
266.893417	760.641297	18.795162	-0.049841	1.672364
266.777505	752.755010	18.800167	-0.049815	1.665689
266.729017	744.909153	18.805171	-0.049800	1.659031
266.611575	737.055971	18.810176	-0.049773	1.652330
266.419318	729.192850	18.815181	-0.049732	1.645583
266.355010	721.360944	18.820186	-0.049715	1.638853
266.346850	713.452641	18.825191	-0.049709	1.632037
266.352905	705.554883	18.830195	-0.049705	1.625204
266.263618	697.718973	18.835200	-0.049683	1.618382
266.237420	689.852113	18.840205	-0.049673	1.611513
266.266618	681.996535	18.845210	-0.049673	1.604632
265.941443	674.197317	18.850215	-0.049607	1.597721
266.096496	666.312429	18.855219	-0.049631	1.590773
266.001849	658.473359	18.860224	-0.049608	1.583799
265.907111	650.645283	18.865229	-0.049586	1.576804
266.053761	642.765895	18.870234	-0.049608	1.569766
265.912459	634.948050	18.875239	-0.049576	1.562711
265.752927	627.151479	18.880243	-0.049541	1.555640
265.637057	619.298142	18.885248	-0.049515	1.548492
265.589082	611.462937	18.890253	-0.049501	1.541337
265.501517	603.651480	18.895258	-0.049479	1.534164
265.554029	595.781418	18.900263	-0.049484	1.526925
265.631202	587.954280	18.905267	-0.049493	1.519695
265.585088	580.133543	18.910272	-0.049479	1.512417
265.457323	572.310550	18.915277	-0.049450	1.505090
265.471277	564.506386	18.920282	-0.049448	1.497766
265.397795	556.683100	18.925287	-0.049429	1.490375
265.240951	548.897147	18.930291	-0.049395	1.482969
265.332310	541.073720	18.935296	-0.049407	1.475529
265.135460	533.227881	18.940301	-0.049365	1.467985
265.307619	525.395717	18.945306	-0.049392	1.460473
264.909179	517.660659	18.950311	-0.049312	1.452925
265.200692	509.800265	18.955315	-0.049361	1.445327
265.000820	502.046902	18.960320	-0.049319	1.437714
264.973332	494.241686	18.965325	-0.049309	1.430037
264.934291	486.458944	18.970330	-0.049297	1.422339
264.704657	478.705916	18.975335	-0.049249	1.414598
264.923216	470.872853	18.980339	-0.049284	1.406808
264.756792	463.129223	18.985344	-0.049248	1.399000
264.659823	455.347442	18.990349	-0.049225	1.391122
264.741645	447.546497	18.995354	-0.049235	1.383209
264.548779	439.805320	19.000359	-0.049194	1.375266
264.374929	432.049951	19.005363	-0.049157	1.367265
264.381557	424.280645	19.010368	-0.049153	1.359233
264.375455	416.510453	19.015373	-0.049147	1.351150
264.414890	408.746591	19.020378	-0.049149	1.343034
264.382640	400.999391	19.025383	-0.049138	1.334873
264.343419	393.252807	19.030387	-0.049125	1.326661
264.125949	385.550017	19.035392	-0.049080	1.318413
264.101408	377.711087	19.040397	-0.049070	1.310001
264.054602	369.946082	19.045402	-0.049056	1.301611
263.855025	362.250867	19.050407	-0.049014	1.293214
263.785842	354.539337	19.055411	-0.048996	1.284769
263.715403	346.834769	19.060416	-0.048978	1.276275
263.589589	339.120494	19.065421	-0.048949	1.267703
263.563841	331.424352	19.070426	-0.048940	1.259112
263.607150	323.698772	19.075431	-0.048943	1.250442
263.600556	316.009318	19.080435	-0.048936	1.241743
263.455587	308.333590	19.085440	-0.048904	1.232971
263.293475	300.645468	19.090445	-0.048869	1.224119
263.252046	292.975827	19.095450	-0.048856	1.215247
263.005581	285.316153	19.100455	-0.048805	1.206281
262.954010	277.662474	19.105459	-0.048791	1.197294
262.939427	269.980012	19.110464	-0.048783	1.188212
262.980681	262.310320	19.115469	-0.048786	1.179086
263.036231	254.650290	19.120474	-0.048791	1.169905
262.879195	247.031323	19.125479	-0.048757	1.160656
262.849734	239.385545	19.130483	-0.048746	1.151327
262.739214	231.740238	19.135488	-0.048721	1.141905
262.614740	224.136964	19.140493	-0.048692	1.132454
262.762794	216.500145	19.145498	-0.048715	1.122940
262.411042	208.951381	19.150503	-0.048644	1.113347
262.574177	201.317354	19.155507	-0.048670	1.103675
262.490780	193.744432	19.160512	-0.048649	1.093942
262.298578	186.187824	19.165517	-0.048609	1.084118
262.277492	178.634358	19.170522	-0.048600	1.074247
262.178341	171.064046	19.175527	-0.048576	1.064244
262.321706	163.494502	19.180531	-0.048598	1.054204
262.054462	155.985381	19.185536	-0.048543	1.044052
261.941294	148.482638	19.190541	-0.048517	1.033846
262.055897	140.942116	19.195546	-0.048534	1.023540
261.747648	133.486570	19.200551	-0.048471	1.013146
261.751942	125.987267	19.205555	-0.048467	1.002658
261.611049	118.516836	19.210560	-0.048436	0.992065
261.554437	111.023355	19.215565	-0.048421	0.981346
261.324073	103.606259	19.220570	-0.048373	0.970574
261.335254	96.152862	19.225575	-0.048370	0.959691
261.169805	88.751806	19.230579	-0.048334	0.948714
261.087183	81.346880	19.235584	-0.048314	0.937625
261.095307	73.943466	19.240589	-0.048311	0.926430
261.130268	66.574708	19.245594	-0.048312	0.915158
260.883662	59.464158	19.250599	-0.048262	0.904071