Fri Mar 12 11:52:21 2021


Number of Points = 3624

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.932669	0.115259	0.000000	0.000021	0.720879
0.727239	0.149133	0.005005	0.000059	0.720874
1.140166	0.047785	0.010010	-0.000017	0.720819
1.076684	-0.085295	0.015014	-0.000005	0.720535
0.899922	-0.048041	0.020019	0.000027	0.720546
0.985604	-0.065372	0.025024	0.000012	0.720542
1.014712	-0.071835	0.030029	0.000006	0.720539
0.952097	-0.057128	0.035034	0.000018	0.720546
0.775717	-0.030408	0.040038	0.000051	0.720537
0.928894	-0.052940	0.045043	0.000022	0.720546
0.781234	-0.029232	0.050048	0.000050	0.720541
0.808244	-0.036115	0.055053	0.000045	0.720537
0.809450	-0.033011	0.060058	0.000045	0.720543
0.660005	-0.011959	0.065062	0.000072	0.720532
0.765334	-0.026129	0.070067	0.000053	0.720541
0.781557	-0.032042	0.075072	0.000050	0.720535
0.977564	-0.069298	0.080077	0.000013	0.720531
0.915176	-0.191459	0.085082	0.000025	0.720268
0.866398	-0.208700	0.090086	0.000034	0.720217
1.121825	-0.250237	0.095091	-0.000013	0.720225
1.146889	-0.255940	0.100096	-0.000018	0.720222
0.968121	-0.223600	0.105101	0.000015	0.720223
1.037555	-0.232093	0.110106	0.000002	0.720231
1.204571	-0.377147	0.115110	-0.000028	0.720004
1.214345	-0.429563	0.120115	-0.000030	0.719904
1.024052	-0.397785	0.125120	0.000005	0.719899
1.050038	-0.401196	0.130125	0.000000	0.719902
1.198685	-0.427284	0.135130	-0.000027	0.719903
0.903532	-0.530087	0.140134	0.000028	0.719596
0.821546	-0.509360	0.145139	0.000043	0.719608
1.101648	-0.563017	0.150144	-0.000009	0.719601
0.850012	-0.518213	0.155149	0.000038	0.719601
0.841332	-0.646481	0.160154	0.000040	0.719345
0.940326	-0.702196	0.165158	0.000021	0.719270
1.011597	-0.711497	0.170163	0.000008	0.719276
0.874782	-0.701507	0.175168	0.000033	0.719248
0.921597	-0.855893	0.180173	0.000025	0.718960
0.991458	-0.864588	0.185178	0.000012	0.718967
0.821126	-0.840711	0.190182	0.000044	0.718954
0.791601	-0.944428	0.195187	0.000049	0.718739
0.882721	-1.008950	0.200192	0.000032	0.718644
0.979673	-1.027652	0.205197	0.000014	0.718641
0.761798	-1.074216	0.210202	0.000055	0.718472
0.858495	-1.155602	0.215206	0.000037	0.718345
0.849933	-1.150057	0.220211	0.000039	0.718353
0.828215	-1.261158	0.225216	0.000043	0.718126
0.818266	-1.316566	0.230221	0.000045	0.718013
0.873621	-1.323118	0.235226	0.000034	0.718020
0.436018	-1.400450	0.240230	0.000116	0.717713
0.583427	-1.429284	0.245235	0.000089	0.717708
0.818492	-1.515073	0.250240	0.000045	0.717621
0.704363	-1.614924	0.255245	0.000066	0.717383
0.664215	-1.606284	0.260250	0.000074	0.717386
0.724786	-1.739818	0.265254	0.000063	0.717143
0.519160	-1.731137	0.270259	0.000101	0.717088
0.563892	-1.799595	0.275264	0.000093	0.716968
0.566381	-1.910407	0.280269	0.000092	0.716750
0.441738	-1.890779	0.285274	0.000116	0.716744
0.372082	-2.031320	0.290278	0.000129	0.716442
0.207688	-1.998342	0.295283	0.000159	0.716449
0.194201	-2.111508	0.300288	0.000162	0.716220
-0.645718	-2.007136	0.305293	0.000318	0.716130
-0.663552	-2.034031	0.310298	0.000322	0.716071
-1.101721	-2.052458	0.315302	0.000403	0.715879
-1.658176	-1.951295	0.320307	0.000507	0.715883
-1.651313	-2.047830	0.325312	0.000506	0.715694
-2.664940	-1.944281	0.330317	0.000694	0.715542
-2.544370	-1.962110	0.335322	0.000672	0.715549
-2.741542	-1.993599	0.340326	0.000709	0.715417
-3.330277	-1.980896	0.345331	0.000818	0.715234
-3.171003	-2.010934	0.350336	0.000789	0.715231
-3.540971	-1.949168	0.355341	0.000858	0.715222
-3.874990	-2.046755	0.360346	0.000920	0.714910
-4.227853	-1.988072	0.365350	0.000986	0.714902
-4.482237	-1.939578	0.370355	0.001033	0.714908
-3.926650	-2.079076	0.375360	0.000930	0.714828
-5.204971	-1.963723	0.380365	0.001168	0.714605
-5.315164	-1.939936	0.385370	0.001188	0.714613
-5.458468	-1.919841	0.390374	0.001215	0.714602
-4.979672	-2.001378	0.395379	0.001126	0.714610
-5.776935	-2.018060	0.400384	0.001274	0.714294
-6.332522	-1.930091	0.405389	0.001378	0.714272
-5.859622	-2.008302	0.410394	0.001290	0.714284
-5.906314	-2.006910	0.415398	0.001298	0.714270
-6.456429	-1.933784	0.420403	0.001401	0.714221
-7.026727	-1.958602	0.425408	0.001507	0.713970
-6.720876	-2.016561	0.430413	0.001450	0.713963
-6.956524	-1.969129	0.435418	0.001494	0.713974
-7.225522	-1.925810	0.440422	0.001544	0.713964
-6.845527	-1.993796	0.445427	0.001473	0.713964
-7.697747	-1.998606	0.450432	0.001632	0.713652
-8.209799	-1.910370	0.455437	0.001727	0.713646
-7.773123	-1.981861	0.460442	0.001646	0.713659
-7.784608	-1.984969	0.465446	0.001648	0.713649
-8.096646	-1.926519	0.470451	0.001707	0.713654
-7.906096	-1.998165	0.475456	0.001671	0.713579
-8.668537	-1.974892	0.480461	0.001813	0.713355
-8.617532	-1.980263	0.485466	0.001804	0.713363
-9.182080	-1.885064	0.490470	0.001909	0.713352
-8.814030	-1.947080	0.495475	0.001840	0.713359
-8.719524	-1.963223	0.500480	0.001823	0.713360
-9.257262	-1.896069	0.505485	0.001923	0.713303
-9.479569	-1.996401	0.510490	0.001964	0.713025
-9.459340	-2.001506	0.515494	0.001961	0.713022
-10.106399	-1.885365	0.520499	0.002081	0.713023
-9.596991	-1.975825	0.525504	0.001986	0.713024
-9.446389	-2.005572	0.530509	0.001958	0.713018
-9.564913	-1.981759	0.535514	0.001980	0.713023
-10.227416	-2.024614	0.540518	0.002104	0.712703
-10.298071	-2.008821	0.545523	0.002117	0.712709
-10.617115	-1.950966	0.550528	0.002176	0.712711
-10.688009	-1.942736	0.555533	0.002190	0.712702
-10.492662	-1.971830	0.560538	0.002153	0.712714
-10.706542	-1.938593	0.565542	0.002193	0.712704
-10.743000	-2.021478	0.570547	0.002200	0.712526
-11.465368	-1.961748	0.575552	0.002334	0.712388
-11.423731	-1.969923	0.580557	0.002327	0.712387
-11.333035	-1.981862	0.585562	0.002310	0.712395
-11.766382	-1.910301	0.590566	0.002391	0.712384
-11.511207	-1.950921	0.595571	0.002343	0.712393
-11.543324	-1.947207	0.600576	0.002349	0.712389
-12.208256	-1.946271	0.605581	0.002473	0.712155
-12.361540	-1.950304	0.610586	0.002501	0.712093
-12.188178	-1.986493	0.615590	0.002469	0.712082
-12.493900	-1.927798	0.620595	0.002526	0.712090
-12.362718	-1.951027	0.625600	0.002502	0.712091
-12.332496	-1.959557	0.630605	0.002496	0.712084
-12.074001	-2.000849	0.635610	0.002448	0.712094
-12.950540	-2.006591	0.640614	0.002611	0.711771
-13.403947	-1.928746	0.645619	0.002696	0.711765
-13.358500	-1.936541	0.650624	0.002687	0.711766
-13.404385	-1.932526	0.655629	0.002696	0.711757
-13.317074	-1.943044	0.660634	0.002680	0.711767
-13.233707	-1.962256	0.665638	0.002664	0.711758
-13.457418	-1.921425	0.670643	0.002706	0.711760
-13.483419	-2.028044	0.675648	0.002711	0.711538
-14.464430	-1.897152	0.680653	0.002893	0.711451
-14.155697	-1.947755	0.685658	0.002836	0.711460
-14.346533	-1.918965	0.690662	0.002872	0.711449
-14.402042	-1.907675	0.695667	0.002882	0.711452
-13.998121	-1.977119	0.700672	0.002807	0.711457
-14.695561	-1.857350	0.705677	0.002937	0.711448
-14.483121	-1.959149	0.710682	0.002897	0.711320
-15.473560	-1.876860	0.715686	0.003082	0.711132
-15.200260	-1.922014	0.720691	0.003031	0.711139
-15.415791	-1.881271	0.725696	0.003071	0.711144
-15.321628	-1.903067	0.730701	0.003053	0.711134
-14.925288	-1.970498	0.735706	0.002980	0.711140
-15.571681	-1.860134	0.740710	0.003100	0.711130
-15.265847	-1.910380	0.745715	0.003043	0.711139
-15.041869	-2.062968	0.750720	0.003001	0.710914
-16.157819	-1.889764	0.755725	0.003209	0.710863
-15.933810	-1.924063	0.760730	0.003167	0.710874
-15.817196	-1.950329	0.765734	0.003146	0.710863
-15.841034	-1.943785	0.770739	0.003150	0.710867
-16.295475	-1.860780	0.775744	0.003235	0.710871
-16.237123	-1.889799	0.780749	0.003224	0.710834
-16.536540	-1.985800	0.785754	0.003280	0.710536
-16.859744	-1.932435	0.790758	0.003340	0.710527
-16.872676	-1.929164	0.795763	0.003343	0.710529
-16.421984	-2.007732	0.800768	0.003259	0.710532
-16.885299	-1.927483	0.805773	0.003345	0.710528
-16.963702	-1.909927	0.810778	0.003360	0.710535
-16.861710	-1.982036	0.815782	0.003341	0.710427
-17.782610	-1.923919	0.820787	0.003512	0.710215
-17.693425	-1.940057	0.825792	0.003496	0.710215
-17.833148	-1.916848	0.830797	0.003522	0.710211
-17.585535	-1.956376	0.835802	0.003476	0.710220
-17.877854	-1.907887	0.840806	0.003530	0.710213
-18.056003	-1.876423	0.845811	0.003563	0.710213
-17.577065	-1.995687	0.850816	0.003474	0.710145
-18.586011	-1.943928	0.855821	0.003662	0.709889
-18.311456	-1.989316	0.860826	0.003611	0.709896
-18.753307	-1.915112	0.865830	0.003693	0.709887
-18.582302	-1.943216	0.870835	0.003661	0.709891
-18.704529	-1.920507	0.875840	0.003684	0.709893
-19.004890	-1.871323	0.880845	0.003740	0.709884
-18.489857	-1.996341	0.885850	0.003644	0.709818
-19.649787	-1.903405	0.890854	0.003860	0.709590
-19.567738	-1.916751	0.895859	0.003845	0.709593
-19.390651	-1.946878	0.900864	0.003812	0.709596
-19.773337	-1.880911	0.905869	0.003883	0.709591
-19.707212	-1.887985	0.910874	0.003871	0.709600
-19.703495	-1.893224	0.915878	0.003870	0.709591
-19.430243	-1.938616	0.920883	0.003819	0.709598
-20.136052	-1.971821	0.925888	0.003951	0.709280
-20.621575	-1.894077	0.930893	0.004041	0.709262
-20.507681	-1.909550	0.935898	0.004020	0.709272
-20.561001	-1.906181	0.940902	0.004030	0.709259
-20.812394	-1.860803	0.945907	0.004077	0.709260
-20.370380	-1.936743	0.950912	0.003995	0.709266
-20.526891	-1.912176	0.955917	0.004024	0.709259
-20.548560	-1.997827	0.960922	0.004028	0.709080
-21.573505	-1.877590	0.965926	0.004219	0.708955
-21.300072	-1.926879	0.970931	0.004168	0.708954
-21.354707	-1.916568	0.975936	0.004178	0.708955
-21.693962	-1.859038	0.980941	0.004241	0.708949
-21.214053	-1.938655	0.985946	0.004152	0.708961
-21.321387	-1.924137	0.990950	0.004172	0.708951
-21.565207	-1.962553	0.995955	0.004217	0.708787
-22.219290	-1.917308	1.000960	0.004339	0.708645
-22.312371	-1.904236	1.005965	0.004357	0.708637
-22.354764	-1.894314	1.010970	0.004365	0.708642
-22.477134	-1.875788	1.015974	0.004387	0.708636
-22.179988	-1.928096	1.020979	0.004332	0.708637
-22.333697	-1.897633	1.025984	0.004361	0.708643
-22.692933	-1.863037	1.030989	0.004428	0.708584
-22.605820	-1.990969	1.035994	0.004411	0.708359
-22.790701	-1.963286	1.040998	0.004446	0.708348
-23.513443	-1.834052	1.046003	0.004580	0.708349
-22.894346	-1.942536	1.051008	0.004465	0.708352
-23.020061	-1.924503	1.056013	0.004489	0.708344
-23.009495	-1.921606	1.061018	0.004487	0.708353
-23.237827	-1.974352	1.066022	0.004529	0.708166
-24.232396	-1.873371	1.071027	0.004714	0.708013
-23.924312	-1.926698	1.076032	0.004657	0.708016
-24.094351	-1.899477	1.081037	0.004689	0.708010
-24.065057	-1.901010	1.086042	0.004683	0.708017
-24.056085	-1.906863	1.091046	0.004682	0.708008
-24.146614	-1.890310	1.096051	0.004699	0.708009
-23.768645	-2.006506	1.101056	0.004628	0.707911
-24.865735	-1.918508	1.106061	0.004833	0.707696
-24.657368	-1.951261	1.111066	0.004794	0.707704
-24.860133	-1.916998	1.116070	0.004832	0.707700
-24.801032	-1.928166	1.121075	0.004821	0.707699
-24.809673	-1.925158	1.126080	0.004822	0.707702
-25.528534	-1.801746	1.131085	0.004956	0.707693
-24.814830	-1.987061	1.136090	0.004823	0.707576
-25.870758	-1.900197	1.141094	0.005020	0.707373
-25.787927	-1.915361	1.146099	0.005005	0.707372
-25.709885	-1.926248	1.151104	0.004990	0.707378
-25.707509	-1.931738	1.156109	0.004990	0.707367
-25.658868	-1.935285	1.161114	0.004981	0.707378
-26.124242	-1.854212	1.166118	0.005067	0.707374
-25.906216	-1.929761	1.171123	0.005027	0.707300
-26.515881	-1.928150	1.176128	0.005140	0.707085
-26.759924	-1.890686	1.181133	0.005186	0.707073
-26.699983	-1.897299	1.186138	0.005175	0.707081
-26.771147	-1.886802	1.191142	0.005188	0.707077
-26.880371	-1.864933	1.196147	0.005208	0.707081
-26.621986	-1.909406	1.201152	0.005160	0.707085
-26.706317	-1.901966	1.206157	0.005176	0.707069
-27.270000	-1.958568	1.211162	0.005281	0.706754
-27.777265	-1.871033	1.216166	0.005375	0.706748
-27.799625	-1.864143	1.221171	0.005380	0.706754
-27.293352	-1.953660	1.226176	0.005285	0.706755
-27.892699	-1.850838	1.231181	0.005397	0.706747
-27.617097	-1.895856	1.236186	0.005346	0.706755
-27.405103	-1.936569	1.241190	0.005306	0.706749
-28.118620	-1.941216	1.246195	0.005439	0.706484
-28.614317	-1.871044	1.251200	0.005531	0.706448
-28.534795	-1.888376	1.256205	0.005517	0.706441
-28.093106	-1.962265	1.261210	0.005435	0.706451
-28.583576	-1.879002	1.266214	0.005526	0.706443
-28.538325	-1.886147	1.271219	0.005517	0.706444
-28.017058	-1.976863	1.276224	0.005420	0.706449
-29.008899	-1.958314	1.281229	0.005605	0.706131
-29.115643	-1.938442	1.286234	0.005625	0.706132
-29.338587	-1.902632	1.291238	0.005667	0.706124
-29.298212	-1.907704	1.296243	0.005659	0.706129
-29.198708	-1.923938	1.301248	0.005641	0.706132
-29.430050	-1.885738	1.306253	0.005684	0.706125
-29.225241	-1.935729	1.311258	0.005646	0.706098
-29.988742	-1.917750	1.316262	0.005788	0.705861
-29.859414	-1.939689	1.321267	0.005764	0.705863
-29.702972	-1.963940	1.326272	0.005735	0.705870
-30.320158	-1.859827	1.331277	0.005850	0.705858
-29.973611	-1.917035	1.336282	0.005785	0.705867
-30.150056	-1.888735	1.341286	0.005818	0.705861
-30.121539	-1.982844	1.346291	0.005813	0.705682
-31.249869	-1.859568	1.351296	0.006023	0.705525
-31.167443	-1.877802	1.356301	0.006007	0.705518
-30.748125	-1.947599	1.361306	0.005929	0.705528
-31.234150	-1.862828	1.366310	0.006020	0.705524
-31.193130	-1.870888	1.371315	0.006012	0.705522
-30.827601	-1.934897	1.376320	0.005944	0.705525
-31.256735	-1.905958	1.381325	0.006024	0.705429
-32.012876	-1.876993	1.386330	0.006165	0.705216
-31.783337	-1.921103	1.391334	0.006122	0.705209
-32.336907	-1.822389	1.396339	0.006225	0.705209
-32.172048	-1.849928	1.401344	0.006195	0.705213
-31.949070	-1.894613	1.406349	0.006153	0.705203
-31.889207	-1.902582	1.411354	0.006142	0.705208
-32.220749	-1.845310	1.416358	0.006204	0.705205
-32.366184	-1.963277	1.421363	0.006231	0.704915
-32.489575	-1.953225	1.426368	0.006254	0.704891
-33.078455	-1.851663	1.431373	0.006364	0.704884
-32.825357	-1.894160	1.436378	0.006317	0.704889
-32.637428	-1.929495	1.441382	0.006282	0.704885
-32.566177	-1.944494	1.446387	0.006269	0.704881
-32.838334	-1.918964	1.451392	0.006319	0.704834
-33.911663	-1.852371	1.456397	0.006519	0.704583
-33.492817	-1.922947	1.461402	0.006441	0.704591
-33.716083	-1.883890	1.466406	0.006483	0.704589
-33.833235	-1.863905	1.471411	0.006505	0.704588
-33.432550	-1.933103	1.476416	0.006430	0.704592
-33.881243	-1.856723	1.481421	0.006514	0.704585
-33.779850	-1.870820	1.486426	0.006495	0.704593
-34.116894	-1.976177	1.491430	0.006558	0.704259
-34.690940	-1.873574	1.496435	0.006664	0.704260
-34.833515	-1.845804	1.501440	0.006691	0.704264
-34.425144	-1.923382	1.506445	0.006615	0.704255
-34.316686	-1.939670	1.511450	0.006595	0.704261
-34.641008	-1.884879	1.516454	0.006655	0.704254
-34.496587	-1.925504	1.521459	0.006628	0.704224
-34.759251	-2.014157	1.526464	0.006677	0.703951
-35.290273	-1.922433	1.531469	0.006776	0.703945
-35.782366	-1.832272	1.536474	0.006868	0.703950
-35.215122	-1.936820	1.541478	0.006762	0.703943
-35.116785	-1.954401	1.546483	0.006744	0.703943
-35.375999	-1.903205	1.551488	0.006792	0.703953
-35.525756	-1.949338	1.556493	0.006820	0.703806
-36.044629	-1.940901	1.561498	0.006917	0.703636
-35.909407	-1.967109	1.566502	0.006892	0.703632
-36.166183	-1.922885	1.571507	0.006940	0.703629
-35.904121	-1.967298	1.576512	0.006891	0.703633
-36.098772	-1.935931	1.581517	0.006927	0.703627
-36.373312	-1.882506	1.586522	0.006978	0.703636
-36.684090	-1.960797	1.591526	0.007036	0.703366
-36.869758	-1.942279	1.596531	0.007071	0.703336
-36.978517	-1.920347	1.601536	0.007091	0.703341
-37.112728	-1.901106	1.606541	0.007116	0.703332
-36.634012	-1.980167	1.611546	0.007027	0.703344
-37.098530	-1.898826	1.616550	0.007113	0.703341
-37.248653	-1.907560	1.621555	0.007141	0.703270
-37.650946	-1.964784	1.626560	0.007216	0.703009
-37.628192	-1.973836	1.631565	0.007212	0.702999
-37.887785	-1.923697	1.636570	0.007261	0.703007
-38.017399	-1.902491	1.641574	0.007285	0.703003
-37.886627	-1.927054	1.646579	0.007260	0.703000
-37.878542	-1.924797	1.651584	0.007259	0.703008
-38.157025	-1.933153	1.656589	0.007311	0.702890
-38.698255	-1.935094	1.661594	0.007412	0.702691
-38.549135	-1.963354	1.666598	0.007384	0.702688
-38.928621	-1.896512	1.671603	0.007454	0.702686
-38.702680	-1.934297	1.676608	0.007412	0.702691
-38.710709	-1.937704	1.681613	0.007414	0.702681
-39.046442	-1.872483	1.686618	0.007477	0.702692
-38.979250	-1.933718	1.691622	0.007464	0.702593
-39.679665	-1.921244	1.696627	0.007595	0.702365
-39.319476	-1.982699	1.701632	0.007528	0.702371
-39.985591	-1.869187	1.706637	0.007651	0.702360
-39.722922	-1.912172	1.711642	0.007603	0.702368
-39.345564	-1.980935	1.716646	0.007532	0.702365
-39.978625	-1.869919	1.721651	0.007650	0.702361
-39.842135	-1.925459	1.726656	0.007625	0.702298
-40.312044	-1.957006	1.731661	0.007712	0.702065
-40.326253	-1.950006	1.736666	0.007715	0.702074
-40.705559	-1.885084	1.741670	0.007786	0.702068
-40.515000	-1.920848	1.746675	0.007750	0.702064
-40.114345	-1.988710	1.751680	0.007676	0.702072
-40.835739	-1.863870	1.756685	0.007810	0.702064
-40.702571	-1.956578	1.761690	0.007785	0.701924
-41.490018	-1.906290	1.766694	0.007932	0.701742
-41.614000	-1.884925	1.771699	0.007955	0.701740
-41.679970	-1.870549	1.776704	0.007967	0.701746
-41.518242	-1.904296	1.781709	0.007937	0.701736
-41.313725	-1.935607	1.786714	0.007899	0.701746
-41.507075	-1.903454	1.791718	0.007935	0.701741
-41.615612	-1.898034	1.796723	0.007956	0.701713
-41.983795	-1.967318	1.801728	0.008024	0.701440
-42.641951	-1.856020	1.806733	0.008147	0.701427
-42.774509	-1.829116	1.811738	0.008171	0.701434
-42.144270	-1.943437	1.816742	0.008054	0.701430
-42.466587	-1.887899	1.821747	0.008114	0.701426
-42.419724	-1.892411	1.826752	0.008105	0.701434
-41.996881	-1.971986	1.831757	0.008027	0.701425
-42.757171	-1.984431	1.836762	0.008168	0.701125
-43.387862	-1.875520	1.841766	0.008286	0.701118
-43.539056	-1.849918	1.846771	0.008314	0.701115
-42.851407	-1.969507	1.851776	0.008186	0.701121
-43.409253	-1.874049	1.856781	0.008290	0.701113
-43.373242	-1.877706	1.861786	0.008283	0.701119
-43.003310	-1.944338	1.866790	0.008214	0.701117
-43.547404	-1.967878	1.871795	0.008316	0.700873
-43.991132	-1.888876	1.876800	0.008398	0.700873
-43.876056	-1.912759	1.881805	0.008377	0.700866
-43.710559	-1.939007	1.886810	0.008346	0.700872
-43.917629	-1.901475	1.891814	0.008385	0.700874
-44.010803	-1.886141	1.896819	0.008402	0.700871
-43.620003	-2.046469	1.901824	0.008329	0.700687
-45.057288	-1.868568	1.906829	0.008597	0.700528
-44.591588	-1.948277	1.911834	0.008510	0.700535
-44.468420	-1.971022	1.916838	0.008488	0.700533
-45.177714	-1.847046	1.921843	0.008620	0.700528
-44.818026	-1.907696	1.926848	0.008553	0.700535
-44.790675	-1.916665	1.931853	0.008548	0.700527
-45.162074	-1.991481	1.936858	0.008617	0.700241
-45.916605	-1.869441	1.941862	0.008757	0.700215
-45.968465	-1.861396	1.946867	0.008767	0.700213
-45.219299	-1.989504	1.951872	0.008628	0.700224
-45.896528	-1.874399	1.956877	0.008754	0.700212
-46.038464	-1.845980	1.961882	0.008780	0.700219
-45.583958	-1.927120	1.966886	0.008695	0.700218
-46.257831	-1.962161	1.971891	0.008821	0.699904
-46.619698	-1.901098	1.976896	0.008888	0.699896
-46.917843	-1.851746	1.981901	0.008944	0.699889
-46.232303	-1.971398	1.986906	0.008816	0.699894
-46.548793	-1.914466	1.991910	0.008875	0.699895
-46.913637	-1.850565	1.996915	0.008943	0.699892
-46.661004	-1.958911	2.001920	0.008896	0.699764
-47.203215	-1.943626	2.011917	0.008997	0.699598
-47.354323	-1.915043	2.021914	0.009025	0.699602
-47.317404	-1.923149	2.031910	0.009019	0.699598
-47.701028	-1.854291	2.041907	0.009090	0.699599
-47.190806	-1.946768	2.051904	0.008995	0.699596
-47.450598	-1.899764	2.061901	0.009044	0.699597
-47.343384	-1.919136	2.071898	0.009024	0.699597
-47.394012	-1.910743	2.081894	0.009033	0.699595
-47.273631	-1.933388	2.091891	0.009011	0.699593
-47.309520	-1.925853	2.101888	0.009018	0.699595
-47.361718	-1.915024	2.111885	0.009027	0.699598
-47.063453	-1.877334	2.121882	0.008972	0.699782
-46.780811	-1.872998	2.131878	0.008919	0.699893
-46.777078	-1.874416	2.141875	0.008919	0.699892
-46.330042	-1.954044	2.151872	0.008836	0.699892
-46.572230	-1.909602	2.161869	0.008881	0.699894
-46.299904	-1.916360	2.171866	0.008830	0.699979
-45.674356	-1.910897	2.181862	0.008714	0.700216
-45.613626	-1.922287	2.191859	0.008702	0.700215
-45.668938	-1.911634	2.201856	0.008713	0.700216
-45.629036	-1.919271	2.211853	0.008705	0.700215
-45.059060	-1.893177	2.221850	0.008599	0.700474
-44.903229	-1.892615	2.231846	0.008570	0.700532
-44.923253	-1.889257	2.241843	0.008574	0.700531
-44.676070	-1.931893	2.251840	0.008528	0.700534
-44.362086	-1.835827	2.261837	0.008470	0.700842
-43.797743	-1.920671	2.271834	0.008365	0.700874
-43.872995	-1.908776	2.281830	0.008379	0.700871
-43.884536	-1.893471	2.291827	0.008381	0.700897
-43.251055	-1.896586	2.301824	0.008263	0.701120
-43.269977	-1.891650	2.311821	0.008267	0.701123
-43.268369	-1.893076	2.321818	0.008266	0.701120
-42.861483	-1.852042	2.331814	0.008191	0.701350
-42.455267	-1.884007	2.341811	0.008115	0.701432
-42.552354	-1.865364	2.351808	0.008133	0.701435
-42.294161	-1.843864	2.361805	0.008085	0.701571
-41.305807	-1.935788	2.371802	0.007901	0.701742
-41.848342	-1.840264	2.381798	0.008002	0.701739
-41.424429	-1.911472	2.391795	0.007923	0.701748
-40.737937	-1.874323	2.401792	0.007796	0.702071
-40.647996	-1.890845	2.411789	0.007779	0.702070
-40.458124	-1.924683	2.421786	0.007744	0.702069
-40.456519	-1.857828	2.431782	0.007743	0.702205
-39.482367	-1.954168	2.441779	0.007562	0.702361
-39.829384	-1.891037	2.451776	0.007627	0.702364
-39.760844	-1.902158	2.461773	0.007614	0.702366
-38.858329	-1.918651	2.471770	0.007446	0.702658
-39.012889	-1.877925	2.481766	0.007475	0.702684
-38.870411	-1.903312	2.491763	0.007449	0.702684
-38.736517	-1.865244	2.501760	0.007424	0.702809
-37.853425	-1.928053	2.511757	0.007259	0.703000
-37.969793	-1.907480	2.521754	0.007281	0.703000
-37.979078	-1.906155	2.531750	0.007283	0.702999
-37.248192	-1.894303	2.541747	0.007147	0.703286
-37.168194	-1.883387	2.551744	0.007132	0.703337
-37.013440	-1.908715	2.561741	0.007103	0.703341
-36.949131	-1.868246	2.571738	0.007091	0.703446
-36.196929	-1.910526	2.581734	0.006951	0.703631
-36.137546	-1.921135	2.591731	0.006940	0.703631
-36.059111	-1.934869	2.601728	0.006926	0.703631
-35.681170	-1.895518	2.611725	0.006855	0.703847
-35.299784	-1.912664	2.621722	0.006784	0.703949
-35.562293	-1.866115	2.631718	0.006833	0.703948
-35.253585	-1.867777	2.641715	0.006776	0.704056
-34.492543	-1.904334	2.651712	0.006634	0.704256
-34.366401	-1.925061	2.661709	0.006611	0.704259
-34.408064	-1.917693	2.671706	0.006619	0.704259
-33.923877	-1.872595	2.681702	0.006529	0.704524
-33.504914	-1.916942	2.691699	0.006451	0.704585
-33.655735	-1.888834	2.701696	0.006479	0.704587
-33.470239	-1.868593	2.711693	0.006444	0.704694
-32.834378	-1.885759	2.721690	0.006326	0.704888
-32.828648	-1.888470	2.731686	0.006325	0.704884
-32.726833	-1.908195	2.741683	0.006306	0.704881
-32.168866	-1.848836	2.751680	0.006202	0.705201
-31.587877	-1.949986	2.761677	0.006094	0.705206
-32.003465	-1.875298	2.771674	0.006172	0.705207
-31.590646	-1.879768	2.781670	0.006095	0.705346
-30.929564	-1.910653	2.791667	0.005972	0.705521
-30.952288	-1.906856	2.801664	0.005976	0.705520
-30.925620	-1.909146	2.811661	0.005971	0.705525
-30.286392	-1.867109	2.821658	0.005852	0.705839
-30.193512	-1.873507	2.831654	0.005835	0.705859
-30.159405	-1.879258	2.841651	0.005829	0.705859
-29.784049	-1.887162	2.851648	0.005759	0.705978
-29.090792	-1.937186	2.861645	0.005630	0.706126
-29.295130	-1.901403	2.871642	0.005668	0.706124
-29.084673	-1.940612	2.881638	0.005629	0.706121
-28.806314	-1.845033	2.891635	0.005577	0.706413
-28.362028	-1.910912	2.901632	0.005494	0.706439
-28.562118	-1.873632	2.911629	0.005532	0.706442
-28.271390	-1.825396	2.921626	0.005477	0.706643
-27.777101	-1.860653	2.931622	0.005386	0.706749
-27.899001	-1.839062	2.941619	0.005408	0.706749
-27.395634	-1.853552	2.951616	0.005315	0.706900
-26.599987	-1.904824	2.961613	0.005167	0.707082
-26.825294	-1.864140	2.971610	0.005209	0.707083
-26.739424	-1.877560	2.981606	0.005193	0.707086
-26.194219	-1.831515	2.991603	0.005091	0.707374
-25.791194	-1.901583	3.001600	0.005016	0.707377
-26.040217	-1.857528	3.011597	0.005063	0.707376
-25.408833	-1.862312	3.021594	0.004945	0.707592
-25.350999	-1.819968	3.031590	0.004934	0.707698
-24.973325	-1.886839	3.041587	0.004864	0.707699
-25.011103	-1.838199	3.051584	0.004871	0.707783
-24.075594	-1.889482	3.061581	0.004697	0.708014
-24.160636	-1.876139	3.071578	0.004713	0.708010
-24.183737	-1.871536	3.081574	0.004717	0.708011
-23.618728	-1.840869	3.091571	0.004612	0.708274
-23.111489	-1.894638	3.101568	0.004518	0.708348
-23.005658	-1.913912	3.111565	0.004498	0.708347
-23.006117	-1.912253	3.121562	0.004498	0.708350
-22.549330	-1.852045	3.131558	0.004413	0.708633
-22.315880	-1.892309	3.141555	0.004370	0.708636
-22.354221	-1.885146	3.151552	0.004377	0.708636
-22.106473	-1.839805	3.161549	0.004331	0.708816
-21.318542	-1.910584	3.171546	0.004184	0.708955
-21.390915	-1.898761	3.181542	0.004198	0.708953
-21.542300	-1.870826	3.191539	0.004226	0.708954
-20.661020	-1.877591	3.201536	0.004062	0.709255
-20.673435	-1.870948	3.211533	0.004064	0.709264
-20.696948	-1.865685	3.221530	0.004069	0.709266
-20.377934	-1.825108	3.231526	0.004010	0.709461
-19.901106	-1.842833	3.241523	0.003921	0.709595
-19.770835	-1.865524	3.251520	0.003897	0.709596
-19.829626	-1.821034	3.261517	0.003908	0.709664
-18.809398	-1.887345	3.271514	0.003718	0.709895
-18.889556	-1.873433	3.281510	0.003733	0.709894
-18.980258	-1.858229	3.291507	0.003750	0.709892
-18.072524	-1.905036	3.301504	0.003581	0.710122
-17.910063	-1.884775	3.311501	0.003551	0.710220
-17.952062	-1.877117	3.321498	0.003558	0.710220
-17.947867	-1.874718	3.331494	0.003558	0.710226
-17.463695	-1.807524	3.341491	0.003468	0.710533
-16.948589	-1.898050	3.351488	0.003372	0.710535
-17.252761	-1.842849	3.361485	0.003428	0.710537
-16.392406	-1.889512	3.371482	0.003268	0.710750
-16.349092	-1.835954	3.381478	0.003260	0.710872
-16.157219	-1.871773	3.391475	0.003225	0.710869
-16.227477	-1.851563	3.401472	0.003238	0.710884
-15.431412	-1.866622	3.411469	0.003090	0.711137
-15.463924	-1.860889	3.421466	0.003096	0.711137
-15.583330	-1.842022	3.431462	0.003118	0.711132
-14.912138	-1.850568	3.441459	0.002993	0.711353
-14.683758	-1.841061	3.451456	0.002951	0.711453
-14.589936	-1.858036	3.461453	0.002933	0.711453
-14.437193	-1.835044	3.471450	0.002905	0.711553
-13.805227	-1.845857	3.481446	0.002787	0.711756
-13.425324	-1.912163	3.491443	0.002717	0.711758
-13.626173	-1.875964	3.501440	0.002754	0.711759
-12.815023	-1.901341	3.511437	0.002603	0.711997
-12.306725	-1.944407	3.521434	0.002508	0.712091
-12.429422	-1.924684	3.531430	0.002531	0.712087
-12.264911	-1.954412	3.541427	0.002501	0.712086
-11.929062	-1.911670	3.551424	0.002438	0.712290
-11.638598	-1.913859	3.561421	0.002384	0.712389
-11.306141	-1.973158	3.571418	0.002322	0.712388
-11.711463	-1.901312	3.581414	0.002398	0.712388
-10.980595	-1.887541	3.591411	0.002262	0.712674
-10.662496	-1.926225	3.601408	0.002203	0.712710
-10.385925	-1.974623	3.611405	0.002151	0.712712
-10.637563	-1.904568	3.621402	0.002198	0.712762
-9.787928	-1.926091	3.631398	0.002040	0.713020
-9.440956	-1.986128	3.641395	0.001976	0.713023
-9.885628	-1.905900	3.651392	0.002058	0.713025
-9.582449	-1.892388	3.661389	0.002002	0.713160
-8.759408	-1.937069	3.671386	0.001849	0.713362
-8.919344	-1.909617	3.681382	0.001879	0.713360
-8.624493	-1.962133	3.691379	0.001824	0.713360
-8.290879	-1.910306	3.701376	0.001762	0.713581
-8.064313	-1.913473	3.711373	0.001720	0.713655
-7.836891	-1.953738	3.721370	0.001677	0.713655
-7.949327	-1.902635	3.731366	0.001698	0.713717
-7.224608	-1.906075	3.741363	0.001563	0.713967
-7.190522	-1.912092	3.751360	0.001557	0.713967
-7.007771	-1.943297	3.761357	0.001523	0.713969
-6.562475	-1.902807	3.771354	0.001440	0.714207
-6.383115	-1.900872	3.781350	0.001407	0.714275
-6.095217	-1.952736	3.791347	0.001353	0.714273
-6.265598	-1.876408	3.801344	0.001385	0.714365
-4.995451	-1.980477	3.811341	0.001149	0.714607
-5.378074	-1.911546	3.821338	0.001220	0.714609
-5.217036	-1.940927	3.831334	0.001190	0.714607
-4.810110	-1.924001	3.841331	0.001114	0.714784
-4.215336	-1.968517	3.851328	0.001004	0.714906
-4.343140	-1.944510	3.861325	0.001028	0.714909
-4.355339	-1.941217	3.871322	0.001030	0.714911
-3.695201	-1.917360	3.881318	0.000907	0.715191
-3.585479	-1.918688	3.891315	0.000887	0.715227
-3.575218	-1.919593	3.901312	0.000885	0.715229
-3.095489	-1.940260	3.911309	0.000796	0.715357
-2.535427	-1.945625	3.921306	0.000691	0.715545
-2.576082	-1.939626	3.931302	0.000699	0.715542
-2.660237	-1.925327	3.941299	0.000715	0.715540
-2.056822	-1.901640	3.951296	0.000602	0.715800
-1.651304	-1.930721	3.961293	0.000527	0.715886
-1.800175	-1.905131	3.971290	0.000555	0.715884
-1.558033	-1.922377	3.981286	0.000510	0.715935
-1.390070	-1.853629	3.991283	0.000479	0.716130
-1.255674	-1.876409	4.001280	0.000454	0.716133
-1.320268	-1.827129	4.011277	0.000466	0.716207
-1.177590	-1.731303	4.021274	0.000439	0.716447
-1.071105	-1.750176	4.031270	0.000419	0.716447
-1.062851	-1.637746	4.041267	0.000418	0.716673
-1.072104	-1.595453	4.051264	0.000419	0.716753
-0.605306	-1.589733	4.061261	0.000333	0.716929
-0.626545	-1.508396	4.071258	0.000337	0.717082
-0.618107	-1.443590	4.081254	0.000335	0.717213
-0.617236	-1.362406	4.091251	0.000335	0.717374
-0.658270	-1.255636	4.101248	0.000342	0.717571
-0.635894	-1.193860	4.111245	0.000338	0.717700
-0.332533	-1.098393	4.121242	0.000282	0.717996
-0.510806	-0.999297	4.131238	0.000315	0.718129
-0.338435	-0.917926	4.141235	0.000283	0.718350
-0.455226	-0.771480	4.151232	0.000305	0.718598
-0.186890	-0.723798	4.161229	0.000255	0.718786
-0.188182	-0.621217	4.171226	0.000255	0.718988
-0.229912	-0.474041	4.181222	0.000263	0.719264
-0.049266	-0.366455	4.191219	0.000229	0.719539
-0.216350	-0.217270	4.201216	0.000260	0.719774
0.063516	-0.137210	4.211213	0.000208	0.720030
0.033198	0.009763	4.221210	0.000214	0.720309
-0.005023	0.160659	4.231206	0.000221	0.720593
0.000000	0.349266	4.241203	0.000220	0.720966
0.222013	0.912443	4.246208	0.000178	0.722150
0.460487	2.144052	4.251213	0.000133	0.724649
0.423750	3.993678	4.256218	0.000139	0.728248
1.090477	6.294115	4.261222	0.000013	0.732945
1.023260	9.218274	4.266227	0.000024	0.738560
1.206613	12.576578	4.271232	-0.000013	0.745044
1.590381	16.362158	4.276237	-0.000087	0.752346
1.846044	20.561026	4.281242	-0.000137	0.760306
2.320903	25.130855	4.286246	-0.000228	0.768940
2.813410	30.061807	4.291251	-0.000323	0.778143
3.195591	35.361065	4.296256	-0.000398	0.787865
3.574521	40.986477	4.301261	-0.000472	0.798048
3.952271	46.899364	4.306266	-0.000546	0.808607
4.976466	52.993719	4.311270	-0.000741	0.819541
5.916487	59.384234	4.316275	-0.000920	0.830811
6.470545	66.069109	4.321280	-0.001027	0.842311
6.894443	73.004800	4.326285	-0.001111	0.854034
9.109807	79.822506	4.331290	-0.001528	0.865922
12.576093	86.677335	4.336294	-0.002178	0.878063
13.259460	94.205927	4.341299	-0.002310	0.890330
14.094552	101.866478	4.346304	-0.002470	0.902680
15.624194	109.566582	4.351309	-0.002760	0.915112
16.491432	117.487073	4.356314	-0.002927	0.927537
17.541394	125.520553	4.361318	-0.003127	0.940015
18.727526	133.627786	4.366323	-0.003353	0.952475
19.792111	141.846346	4.371328	-0.003557	0.964905
20.726766	150.171159	4.376333	-0.003736	0.977298
22.321365	158.453731	4.381338	-0.004039	0.989639
23.220126	166.926291	4.386342	-0.004212	1.001925
23.863457	175.453943	4.391347	-0.004337	1.014076
24.633038	183.996548	4.396352	-0.004486	1.026134
25.439851	192.584439	4.401357	-0.004642	1.038122
26.087373	201.203934	4.406362	-0.004768	1.049979
27.043431	209.813637	4.411366	-0.004951	1.061760
27.817948	218.474832	4.416371	-0.005101	1.073439
28.642779	227.102326	4.421376	-0.005260	1.084958
29.363463	235.782514	4.426381	-0.005400	1.096401
29.849409	244.478249	4.431386	-0.005496	1.107694
30.774993	253.127800	4.436390	-0.005674	1.118909
31.403778	261.802141	4.441395	-0.005797	1.129980
32.036329	270.479338	4.446400	-0.005920	1.140948
32.832130	279.153153	4.451405	-0.006074	1.151841
33.328609	287.827709	4.456410	-0.006172	1.162570
33.899103	296.482355	4.461414	-0.006284	1.173192
34.505497	305.096200	4.466419	-0.006402	1.183676
35.186487	313.701909	4.471424	-0.006535	1.194074
36.054062	322.258660	4.476429	-0.006702	1.204361
36.728545	330.846288	4.481434	-0.006833	1.214559
37.065007	339.477286	4.486438	-0.006901	1.224655
37.802073	348.036554	4.491443	-0.007044	1.234664
38.606368	356.540430	4.496448	-0.007199	1.244542
39.366540	365.068048	4.501453	-0.007346	1.254360
39.588569	373.648189	4.506458	-0.007393	1.264059
40.362865	382.146778	4.511462	-0.007543	1.273696
41.185413	390.592007	4.516467	-0.007702	1.283211
41.822182	399.075354	4.521472	-0.007826	1.292663
42.560818	407.540498	4.526477	-0.007969	1.302045
43.330463	416.049869	4.531482	-0.008118	1.311413
43.770377	424.583963	4.536486	-0.008205	1.320681
44.467765	432.981634	4.541491	-0.008340	1.329785
45.137699	441.389737	4.546496	-0.008471	1.338833
45.569658	449.823197	4.551501	-0.008556	1.347805
45.887032	458.266632	4.556506	-0.008621	1.356707
46.384142	466.654352	4.561510	-0.008719	1.365525
47.080567	475.007967	4.566515	-0.008854	1.374285
47.856078	483.339354	4.571520	-0.009004	1.382980
48.751109	491.677138	4.576525	-0.009176	1.391647
49.331877	500.021695	4.581530	-0.009290	1.400214
50.194717	508.333247	4.586534	-0.009456	1.408743
50.855906	516.672551	4.591539	-0.009584	1.417214
51.616452	524.977415	4.596544	-0.009731	1.425617
52.320647	533.327674	4.601549	-0.009868	1.434006
52.817694	541.651909	4.606554	-0.009966	1.442286
53.235775	550.003714	4.611558	-0.010049	1.450534
53.640028	558.354872	4.616563	-0.010129	1.458731
54.408290	566.610144	4.621568	-0.010278	1.466848
55.520799	574.888136	4.626573	-0.010490	1.474996
55.982632	583.178997	4.631578	-0.010582	1.483010
56.529512	591.478798	4.636582	-0.010689	1.491001
57.175654	599.752530	4.641587	-0.010815	1.498941
57.553400	608.047914	4.646592	-0.010890	1.506817
57.987346	616.356736	4.651597	-0.010977	1.514674
58.414770	624.622634	4.656602	-0.011062	1.522449
59.207585	632.848881	4.661606	-0.011214	1.530203
59.804408	641.107019	4.666611	-0.011331	1.537917
60.048743	649.391005	4.671616	-0.011382	1.545564
60.668019	657.655138	4.676621	-0.011502	1.553210
61.217588	665.864920	4.681626	-0.011610	1.560760
61.644043	674.110002	4.686630	-0.011695	1.568286
62.040745	682.363766	4.691635	-0.011774	1.575780
62.545893	690.578797	4.696640	-0.011873	1.583219
63.111277	698.811851	4.701645	-0.011984	1.590648
63.417140	707.055206	4.706650	-0.012046	1.598015
63.953210	715.253861	4.711654	-0.012151	1.605340
64.591227	723.460419	4.716659	-0.012276	1.612654
65.125033	731.657602	4.721664	-0.012380	1.619911
65.403592	739.914742	4.726669	-0.012438	1.627153
66.224669	748.122171	4.731674	-0.012596	1.634394
66.984112	756.268595	4.736678	-0.012742	1.641542
67.423721	764.461498	4.741683	-0.012830	1.648655
68.003737	772.657014	4.746688	-0.012943	1.655758
68.551808	780.851325	4.751693	-0.013050	1.662826
69.097163	789.022851	4.756698	-0.013157	1.669844
69.511290	797.252229	4.761702	-0.013240	1.676863
70.082964	805.411625	4.766707	-0.013351	1.683815
70.460008	813.612881	4.771712	-0.013427	1.690748
70.928018	821.825636	4.776717	-0.013519	1.697674
71.170053	830.025626	4.781722	-0.013570	1.704531
71.681648	838.218529	4.786726	-0.013670	1.711390
72.197965	846.394880	4.791731	-0.013772	1.718209
72.524402	854.548741	4.796736	-0.013838	1.724957
73.098503	862.710726	4.801741	-0.013950	1.731717
73.668088	870.847480	4.806746	-0.014061	1.738430
74.214030	878.987869	4.811750	-0.014168	1.745117
74.884844	887.149228	4.816755	-0.014298	1.751811
75.137237	895.339039	4.821760	-0.014351	1.758449
75.837366	903.459689	4.826765	-0.014486	1.765063
76.697350	911.567477	4.831770	-0.014652	1.771661
77.467339	919.717436	4.836774	-0.014800	1.778257
78.133261	927.858135	4.841779	-0.014930	1.784809
78.226484	936.117717	4.846784	-0.014952	1.791360
78.925686	944.276863	4.851789	-0.015088	1.797882
79.144487	952.430684	4.856794	-0.015134	1.804317
79.304861	960.627284	4.861798	-0.015169	1.810756
79.619060	968.787817	4.866803	-0.015233	1.817163
80.137208	976.891938	4.871808	-0.015335	1.823527
80.571365	985.040650	4.876813	-0.015421	1.829894
80.789188	993.206502	4.881818	-0.015466	1.836226
81.151586	1001.342603	4.886822	-0.015539	1.842530
81.561177	1009.473804	4.891827	-0.015621	1.848815
81.935773	1017.612869	4.896832	-0.015696	1.855080
82.728621	1025.695298	4.901837	-0.015849	1.861329
82.985377	1033.851114	4.906842	-0.015902	1.867551
83.187242	1042.062812	4.911846	-0.015945	1.873788
83.550256	1050.170542	4.916851	-0.016018	1.879945
84.240508	1058.238956	4.921856	-0.016151	1.886089
84.848030	1066.369647	4.926861	-0.016270	1.892250
84.992931	1074.525837	4.931866	-0.016302	1.898358
85.505521	1082.628963	4.936870	-0.016403	1.904447
85.918069	1090.763329	4.941875	-0.016485	1.910530
86.041165	1098.931215	4.946880	-0.016513	1.916585
86.438610	1107.033587	4.951885	-0.016592	1.922603
86.801325	1115.140580	4.956890	-0.016665	1.928603
87.316018	1123.262637	4.961894	-0.016766	1.934611
87.561081	1131.396399	4.966899	-0.016817	1.940579
87.866323	1139.518916	4.971904	-0.016879	1.946527
88.230032	1147.686431	4.976909	-0.016952	1.952496
88.481310	1155.801732	4.981914	-0.017004	1.958397
88.927496	1163.863179	4.986918	-0.017092	1.964263
89.286217	1171.981315	4.991923	-0.017164	1.970142
89.676924	1180.075661	4.996928	-0.017242	1.975990
90.050795	1188.184386	5.001933	-0.017317	1.981828
90.317068	1196.295010	5.006938	-0.017372	1.987640
90.634564	1204.432554	5.011942	-0.017437	1.993459
90.985036	1212.527079	5.016947	-0.017507	1.999234
91.606137	1220.563833	5.021952	-0.017628	2.004980
92.097574	1228.685071	5.026957	-0.017725	2.010755
92.315069	1236.811872	5.031962	-0.017770	2.016489
92.855351	1244.894256	5.036966	-0.017876	2.022209
93.308749	1252.998483	5.041971	-0.017966	2.027919
93.901702	1261.111216	5.046976	-0.018082	2.033633
94.044502	1269.257694	5.051981	-0.018114	2.039309
94.479261	1277.305609	5.056986	-0.018200	2.044930
94.911361	1285.420759	5.061990	-0.018285	2.050581
95.375327	1293.518156	5.066995	-0.018377	2.056208
95.875174	1301.590794	5.072000	-0.018475	2.061806
96.669853	1309.657078	5.077005	-0.018629	2.067414
96.803581	1317.820627	5.082010	-0.018659	2.073007
97.057019	1325.943960	5.087014	-0.018711	2.078570
97.465085	1334.016877	5.092019	-0.018792	2.084098
97.898363	1342.091304	5.097024	-0.018878	2.089616
98.203079	1350.234747	5.102029	-0.018940	2.095152
98.426266	1358.321882	5.107034	-0.018987	2.100629
98.778145	1366.407501	5.112038	-0.019058	2.106102
99.130748	1374.550215	5.117043	-0.019129	2.111599
99.313333	1382.675214	5.122048	-0.019168	2.117054
99.804375	1390.709189	5.127053	-0.019265	2.122464
100.246940	1398.764924	5.132058	-0.019352	2.127869
100.857716	1406.843443	5.137062	-0.019471	2.133292
101.441399	1414.898751	5.142067	-0.019585	2.138683
101.801152	1422.974771	5.147072	-0.019657	2.144053
102.053420	1431.106633	5.152077	-0.019710	2.149436
102.480184	1439.194912	5.157082	-0.019794	2.154793
102.816671	1447.284606	5.162086	-0.019862	2.160130
103.238144	1455.350199	5.167091	-0.019946	2.165445
103.437783	1463.454826	5.172096	-0.019988	2.170752
103.798135	1471.565485	5.177101	-0.020061	2.176065
104.338805	1479.606381	5.182106	-0.020167	2.181336
104.947621	1487.672437	5.187110	-0.020285	2.186616
105.414495	1495.777586	5.192115	-0.020377	2.191896
105.494510	1503.895995	5.197120	-0.020398	2.197137
105.918230	1511.952282	5.202125	-0.020482	2.202356
106.419582	1520.006582	5.207130	-0.020580	2.207569
106.591180	1528.138203	5.212134	-0.020617	2.212789
107.108913	1536.193994	5.217139	-0.020719	2.217979
107.453465	1544.262448	5.222144	-0.020788	2.223150
107.806043	1552.346610	5.227149	-0.020859	2.228319
107.955523	1560.476524	5.232154	-0.020892	2.233487
108.259305	1568.540572	5.237158	-0.020954	2.238616
108.645520	1576.610346	5.242163	-0.021031	2.243743
108.843156	1584.694388	5.247168	-0.021073	2.248851
109.208101	1592.798791	5.252173	-0.021147	2.253974
109.741416	1600.817225	5.257178	-0.021251	2.259047
110.222934	1608.885001	5.262182	-0.021346	2.264135
110.718230	1616.949833	5.267187	-0.021443	2.269210
110.989007	1625.126916	5.272192	-0.021499	2.274325
111.295328	1633.180343	5.277197	-0.021561	2.279354
111.420284	1641.243542	5.282202	-0.021590	2.284363
111.616404	1649.309421	5.287206	-0.021632	2.289368
112.386132	1657.343006	5.292211	-0.021780	2.294391
112.755301	1665.384077	5.297216	-0.021854	2.299374
113.020173	1673.468619	5.302221	-0.021909	2.304364
113.279847	1681.550436	5.307226	-0.021962	2.309340
113.766184	1689.628051	5.312230	-0.022058	2.314323
114.003117	1697.710406	5.317235	-0.022107	2.319276
114.129060	1705.774057	5.322240	-0.022136	2.324199
114.562939	1713.840955	5.327245	-0.022222	2.329138
115.150113	1721.888968	5.332250	-0.022337	2.334068
115.117853	1730.011734	5.337254	-0.022336	2.338982
115.523262	1738.061913	5.342259	-0.022417	2.343878
115.808404	1746.131506	5.347264	-0.022475	2.348765
116.161283	1754.249733	5.352269	-0.022546	2.353677
116.529156	1762.271718	5.357274	-0.022620	2.358522
117.041391	1770.302458	5.362278	-0.022720	2.363373
117.218034	1778.382978	5.367283	-0.022758	2.368218
117.508068	1786.458372	5.372288	-0.022818	2.373058
118.058404	1794.497907	5.377293	-0.022925	2.377888
118.220298	1802.574443	5.382298	-0.022961	2.382700
118.593016	1810.642084	5.387302	-0.023035	2.387512
118.991989	1818.708227	5.392307	-0.023115	2.392317
119.439835	1826.766868	5.397312	-0.023203	2.397111
119.797150	1834.833870	5.402317	-0.023275	2.401893
119.950009	1842.898190	5.407322	-0.023309	2.406648
120.471273	1850.957807	5.412326	-0.023411	2.411419
120.849468	1859.054869	5.417331	-0.023487	2.416192
120.708354	1867.145903	5.422336	-0.023466	2.420912
121.257231	1875.186754	5.427341	-0.023573	2.425646
121.734519	1883.246706	5.432346	-0.023667	2.430377
122.088094	1891.386861	5.437350	-0.023738	2.435135
122.431831	1899.407374	5.442355	-0.023808	2.439814
122.875660	1907.404707	5.447360	-0.023895	2.444478
123.289931	1915.467730	5.452365	-0.023978	2.449169
123.470713	1923.544609	5.457370	-0.024017	2.453841
123.989209	1931.568072	5.462374	-0.024118	2.458499
124.273520	1939.624397	5.467379	-0.024177	2.463149
124.438437	1947.683124	5.472384	-0.024213	2.467783
124.917373	1955.759020	5.477389	-0.024307	2.472441
125.276203	1963.804841	5.482394	-0.024379	2.477065
125.535416	1971.861348	5.487398	-0.024432	2.481678
125.722947	1979.940953	5.492403	-0.024473	2.486291
125.934859	1988.008604	5.497408	-0.024517	2.490890
126.372270	1996.080860	5.502413	-0.024604	2.495499
126.569396	2004.125402	5.507418	-0.024646	2.500067
127.083110	2012.137578	5.512422	-0.024747	2.504631
127.472454	2020.226438	5.517427	-0.024824	2.509221
127.572288	2028.339573	5.522432	-0.024848	2.513795
127.822727	2036.402611	5.527437	-0.024900	2.518344
128.082992	2044.405591	5.532442	-0.024954	2.522851
128.287609	2052.484039	5.537446	-0.024997	2.527389
128.751843	2060.520185	5.542451	-0.025089	2.531913
129.063055	2068.574012	5.547456	-0.025152	2.536428
129.432296	2076.628263	5.552461	-0.025226	2.540940
129.471802	2084.675508	5.557466	-0.025239	2.545416
129.834809	2092.729349	5.562470	-0.025311	2.549910
130.146436	2100.810922	5.567475	-0.025375	2.554408
130.457584	2108.827037	5.572480	-0.025438	2.558863
130.898452	2116.877142	5.577485	-0.025525	2.563337
131.052800	2124.950273	5.582490	-0.025559	2.567796
131.275703	2133.021510	5.587494	-0.025606	2.572251
131.767132	2141.064540	5.592499	-0.025702	2.576701
132.076217	2149.097391	5.597504	-0.025765	2.581125
132.383256	2157.157326	5.602509	-0.025828	2.585557
132.505256	2165.239886	5.607514	-0.025856	2.589980
132.843085	2173.484973	5.612518	-0.025924	2.594499
133.072323	2181.478960	5.617523	-0.025972	2.598866
133.367967	2189.452384	5.622528	-0.026032	2.603220
133.551632	2197.491295	5.627533	-0.026071	2.607593
133.884605	2205.533335	5.632538	-0.026138	2.611972
134.334359	2213.563311	5.637542	-0.026227	2.616344
134.593719	2221.603968	5.642547	-0.026281	2.620701
134.786506	2229.619156	5.647552	-0.026322	2.625034
135.184160	2237.680473	5.652557	-0.026401	2.629397
135.362666	2245.752792	5.657562	-0.026440	2.633745
135.712552	2253.779289	5.662566	-0.026510	2.638072
136.008310	2261.809786	5.667571	-0.026570	2.642390
136.297245	2269.840119	5.672576	-0.026629	2.646701
136.517005	2277.914748	5.677581	-0.026676	2.651024
136.844916	2285.965704	5.682586	-0.026742	2.655334
137.354183	2293.987223	5.687590	-0.026842	2.659633
137.526580	2302.057241	5.692595	-0.026879	2.663930
137.741152	2310.094591	5.697600	-0.026924	2.668204
137.883478	2318.208061	5.702605	-0.026956	2.672508
138.323219	2326.235917	5.707610	-0.027043	2.676778
138.489063	2334.265638	5.712614	-0.027079	2.681025
138.846388	2342.303412	5.717619	-0.027151	2.685281
139.001015	2350.341811	5.722624	-0.027185	2.689518
139.041085	2358.449053	5.727629	-0.027198	2.693778
139.426601	2366.463783	5.732634	-0.027275	2.698004
139.600751	2374.508368	5.737638	-0.027312	2.702225
140.028948	2382.548299	5.742643	-0.027397	2.706454
140.344255	2390.573870	5.747648	-0.027461	2.710661
140.803536	2398.644053	5.752653	-0.027552	2.714894
140.770974	2406.705364	5.757658	-0.027551	2.719085
140.888973	2414.722041	5.762662	-0.027578	2.723255
141.302161	2422.772577	5.767667	-0.027660	2.727455
141.572363	2430.806899	5.772672	-0.027716	2.731632
141.886829	2438.874417	5.777677	-0.027780	2.735822
142.270888	2446.886317	5.782682	-0.027856	2.739980
142.431969	2454.929716	5.787686	-0.027892	2.744135
142.636105	2463.007038	5.792691	-0.027935	2.748304
143.037367	2471.092969	5.797696	-0.028015	2.752483
143.401624	2479.175074	5.802701	-0.028088	2.756651
143.665222	2487.161294	5.807706	-0.028142	2.760758
143.960881	2495.168019	5.812710	-0.028202	2.764871
144.254071	2503.225060	5.817715	-0.028262	2.769003
144.407170	2511.280666	5.822720	-0.028296	2.773120
144.833581	2519.321961	5.827725	-0.028381	2.777240
145.019455	2527.347552	5.832730	-0.028420	2.781331
145.317630	2535.376316	5.837734	-0.028481	2.785425
145.649168	2543.435381	5.842739	-0.028548	2.789530
145.970137	2551.493539	5.847744	-0.028613	2.793627
146.560262	2559.504748	5.852749	-0.028728	2.797711
146.810302	2567.551199	5.857754	-0.028780	2.801786
147.110060	2575.572781	5.862758	-0.028841	2.805846
147.317809	2583.632272	5.867763	-0.028885	2.809914
147.499895	2591.710868	5.872768	-0.028924	2.813984
147.794666	2599.739146	5.877773	-0.028984	2.818029
147.966616	2607.783225	5.882778	-0.029021	2.822069
148.043554	2615.832316	5.887782	-0.029041	2.826100
148.345921	2623.883472	5.892787	-0.029102	2.830140
148.590173	2631.940405	5.897792	-0.029153	2.834173
148.955017	2639.959489	5.902797	-0.029226	2.838189
149.386102	2647.953097	5.907802	-0.029312	2.842190
149.538387	2655.998003	5.912806	-0.029345	2.846195
149.819749	2664.058615	5.917811	-0.029403	2.850209
149.929514	2672.126178	5.922816	-0.029428	2.854211
150.127906	2680.175556	5.927821	-0.029471	2.858204
150.310046	2688.193862	5.932826	-0.029510	2.862175
150.549814	2696.225799	5.937830	-0.029560	2.866150
151.040734	2704.245915	5.942835	-0.029656	2.870128
151.257935	2712.306826	5.947840	-0.029702	2.874105
151.583200	2720.358040	5.952845	-0.029768	2.878078
151.907412	2728.395206	5.957850	-0.029833	2.882038
152.032983	2736.423017	5.962854	-0.029862	2.885977
152.279446	2744.465666	5.967859	-0.029913	2.889925
152.486451	2752.528314	5.972864	-0.029957	2.893875
152.542142	2760.595816	5.977869	-0.029972	2.897814
152.846660	2768.601268	5.982874	-0.030034	2.901730
153.258782	2776.585913	5.987878	-0.030116	2.905637
153.376262	2784.687328	5.992883	-0.030143	2.909580
153.503533	2792.805807	5.997888	-0.030172	2.913526
153.677747	2800.835433	6.002893	-0.030210	2.917426
153.898838	2808.825569	6.007898	-0.030256	2.921304
154.210652	2816.804879	6.012902	-0.030319	2.925176
154.780480	2824.817874	6.017907	-0.030431	2.929073
154.874875	2832.894374	6.022912	-0.030453	2.932971
155.115200	2840.972923	6.027917	-0.030503	2.936872
155.281233	2848.970985	6.032922	-0.030540	2.940725
155.566804	2856.970566	6.037926	-0.030598	2.944580
155.891965	2865.032542	6.042931	-0.030664	2.948462
156.320957	2873.058862	6.047936	-0.030749	2.952327
156.850265	2881.106670	6.052941	-0.030852	2.956202
157.223991	2889.121901	6.057946	-0.030927	2.960049
157.169826	2897.172815	6.062950	-0.030922	2.963886
157.547790	2905.231045	6.067955	-0.030998	2.967743
157.726132	2913.260274	6.072960	-0.031036	2.971571
158.439942	2921.282148	6.077965	-0.031175	2.975418
158.857002	2929.300375	6.082970	-0.031257	2.979243
159.302455	2937.339295	6.087974	-0.031346	2.983074
159.638059	2945.385292	6.092979	-0.031413	2.986899
159.826227	2953.432979	6.097984	-0.031453	2.990711
160.147354	2961.502104	6.102989	-0.031519	2.994536
160.299750	2969.537933	6.107994	-0.031552	2.998331
160.295069	2977.571418	6.112998	-0.031556	3.002113
160.554674	2985.613097	6.118003	-0.031610	3.005907
160.746937	2993.602309	6.123008	-0.031651	3.009668
160.865397	3001.677980	6.128013	-0.031678	3.013461
161.106806	3009.727668	6.133018	-0.031728	3.017243
161.499705	3017.740356	6.138022	-0.031807	3.021011
161.814506	3025.760715	6.143027	-0.031871	3.024773
161.721991	3033.828995	6.148032	-0.031859	3.028534
161.972803	3041.894339	6.153037	-0.031911	3.032305
162.212923	3049.934058	6.158042	-0.031960	3.036059
162.338811	3057.904984	6.163046	-0.031989	3.039771
162.712021	3065.959040	6.168051	-0.032064	3.043528
162.864381	3073.963870	6.173056	-0.032097	3.047248
163.199759	3082.029848	6.178061	-0.032165	3.051000
163.261654	3090.091523	6.183066	-0.032182	3.054732
163.505046	3098.105926	6.188070	-0.032232	3.058447
163.806816	3106.133024	6.193075	-0.032294	3.062165
163.996539	3114.144223	6.198080	-0.032334	3.065867
164.376939	3122.176281	6.203085	-0.032410	3.069582
164.496408	3130.315516	6.208090	-0.032438	3.073330
164.652547	3138.344706	6.213094	-0.032472	3.077025
165.160562	3146.327490	6.218099	-0.032572	3.080710
165.367466	3154.313779	6.223104	-0.032615	3.084378
165.572003	3162.381609	6.228109	-0.032659	3.088080
165.778693	3170.418003	6.233114	-0.032702	3.091762
166.038293	3178.442337	6.238118	-0.032756	3.095437
166.200875	3186.475821	6.243123	-0.032791	3.099107
166.173193	3194.494104	6.248128	-0.032792	3.102757
166.424521	3202.557756	6.253133	-0.032844	3.106437
166.672868	3210.559892	6.258138	-0.032895	3.110083
166.927684	3218.622538	6.263142	-0.032948	3.113754
167.108522	3226.649817	6.268147	-0.032986	3.117400
167.288775	3234.664570	6.273152	-0.033025	3.121037
167.521710	3242.680092	6.278157	-0.033074	3.124672
167.934372	3250.716336	6.283162	-0.033156	3.128320
168.087321	3258.758743	6.288166	-0.033190	3.131955
168.363737	3266.817820	6.293171	-0.033246	3.135598
168.366478	3274.845320	6.298176	-0.033252	3.139211
168.461235	3282.874432	6.303181	-0.033275	3.142825
168.787003	3290.908989	6.308186	-0.033341	3.146447
169.046243	3298.912818	6.313190	-0.033394	3.150049
169.207528	3307.032423	6.318195	-0.033429	3.153693
169.537507	3315.008953	6.323200	-0.033496	3.157277
169.949401	3323.036377	6.328205	-0.033578	3.160883
170.122370	3331.036184	6.333210	-0.033615	3.164462
170.219052	3339.072841	6.338214	-0.033639	3.168050
170.816663	3347.101123	6.343219	-0.033755	3.171652
170.997860	3355.141778	6.348224	-0.033794	3.175237
171.115532	3363.180862	6.353229	-0.033821	3.178815
171.454896	3371.204262	6.358234	-0.033889	3.182391
171.628951	3379.230866	6.363238	-0.033927	3.185958
171.539015	3387.310849	6.368243	-0.033916	3.189533
171.679882	3395.354530	6.373248	-0.033947	3.193098
172.121127	3403.368064	6.378253	-0.034034	3.196658
172.236747	3411.398357	6.383258	-0.034061	3.200207
172.256797	3419.390731	6.388262	-0.034070	3.203732
172.590608	3427.413994	6.393267	-0.034137	3.207280
172.710856	3435.457968	6.398272	-0.034165	3.210824
172.951781	3443.492412	6.403277	-0.034215	3.214365
173.199643	3451.520957	6.408282	-0.034266	3.217900
173.661956	3459.536900	6.413286	-0.034358	3.221434
173.886066	3467.581347	6.418291	-0.034405	3.224967
174.026576	3475.596143	6.423296	-0.034436	3.228480
174.289683	3483.659049	6.428301	-0.034490	3.232014
174.378673	3491.760009	6.433306	-0.034512	3.235555
174.367826	3499.725170	6.438310	-0.034515	3.239028
174.751582	3507.730414	6.443315	-0.034592	3.242531
175.035449	3515.730064	6.448320	-0.034650	3.246023
175.124284	3523.770854	6.453325	-0.034672	3.249522
175.400636	3531.818190	6.458330	-0.034728	3.253028
175.759926	3539.848721	6.463334	-0.034800	3.256525
175.910175	3547.906524	6.468339	-0.034834	3.260022
176.035064	3555.908264	6.473344	-0.034862	3.263491
176.361725	3563.938442	6.478349	-0.034928	3.266975
176.506782	3571.975110	6.483354	-0.034960	3.270452
176.530577	3580.027817	6.488358	-0.034970	3.273927
177.041429	3588.045615	6.493363	-0.035070	3.277403
177.044983	3596.057904	6.498368	-0.035076	3.280852
177.149429	3604.069515	6.503373	-0.035101	3.284302
177.556272	3612.113959	6.508378	-0.035182	3.287773
177.942435	3620.123844	6.513382	-0.035259	3.291226
177.968549	3628.202351	6.518387	-0.035269	3.294690
178.192445	3636.195801	6.523392	-0.035316	3.298121
178.265376	3644.233092	6.528397	-0.035335	3.301562
178.446705	3652.243558	6.533402	-0.035373	3.304993
178.448393	3660.309894	6.538406	-0.035379	3.308436
179.018217	3668.346632	6.543411	-0.035490	3.311885
179.188774	3676.369489	6.548416	-0.035527	3.315309
179.518342	3684.366117	6.553421	-0.035594	3.318725
179.651068	3692.389250	6.558426	-0.035624	3.322141
179.824297	3700.386254	6.563430	-0.035661	3.325543
180.299588	3708.414334	6.568435	-0.035755	3.328967
180.487299	3716.454009	6.573440	-0.035795	3.332381
180.700808	3724.514526	6.578445	-0.035840	3.335801
181.133449	3732.527377	6.583450	-0.035926	3.339206
181.275943	3740.544309	6.588454	-0.035957	3.342599
181.435000	3748.593183	6.593459	-0.035992	3.346002
181.618590	3756.631170	6.598464	-0.036032	3.349397
181.913361	3764.674468	6.603469	-0.036092	3.352796
182.152572	3772.738292	6.608474	-0.036142	3.356198
182.281823	3780.702476	6.613478	-0.036171	3.359550
182.473165	3788.771257	6.618483	-0.036212	3.362945
182.585230	3796.776901	6.623488	-0.036238	3.366308
182.970950	3804.785844	6.628493	-0.036315	3.369678
183.074782	3812.868078	6.633498	-0.036339	3.373065
183.190381	3820.885794	6.638502	-0.036366	3.376423
183.604011	3828.892225	6.643507	-0.036448	3.379783
183.924993	3836.879503	6.648512	-0.036513	3.383128
184.118889	3844.922293	6.653517	-0.036554	3.386488
184.191855	3852.983370	6.658522	-0.036573	3.389849
184.698232	3861.044543	6.663526	-0.036673	3.393221
184.819728	3869.098957	6.668531	-0.036701	3.396574
184.891727	3877.076794	6.673536	-0.036719	3.399890
185.322947	3885.061805	6.678541	-0.036805	3.403218
185.595649	3893.077853	6.683546	-0.036861	3.406550
185.644950	3901.100097	6.688550	-0.036875	3.409874
185.705629	3909.172292	6.693555	-0.036892	3.413215
185.971328	3917.183313	6.698560	-0.036946	3.416535
186.201052	3925.195394	6.703565	-0.036994	3.419851
186.660253	3933.198733	6.708570	-0.037085	3.423168
186.803105	3941.221654	6.713574	-0.037117	3.426479
186.981129	3949.259390	6.718579	-0.037155	3.429794
187.018458	3957.318779	6.723584	-0.037167	3.433110
187.253737	3965.375913	6.728589	-0.037216	3.436428
187.720218	3973.361254	6.733594	-0.037308	3.439721
187.896034	3981.371225	6.738598	-0.037346	3.443012
188.288413	3989.416384	6.743603	-0.037424	3.446321
188.463525	3997.391633	6.748608	-0.037462	3.449591
188.769751	4005.485422	6.753613	-0.037525	3.452911
188.993241	4013.538754	6.758618	-0.037571	3.456208
189.205995	4021.526509	6.763622	-0.037616	3.459475
189.401622	4029.550104	6.768627	-0.037658	3.462752
189.529251	4037.562291	6.773632	-0.037687	3.466020
189.725720	4045.603486	6.778637	-0.037729	3.469299
189.963443	4053.684449	6.783642	-0.037778	3.472592
190.056148	4061.708564	6.788646	-0.037800	3.475854
190.223347	4069.684346	6.793651	-0.037837	3.479096
190.588542	4077.696719	6.798656	-0.037910	3.482356
190.768465	4085.693566	6.803661	-0.037949	3.485601
191.082611	4093.739909	6.808666	-0.038012	3.488867
191.268970	4101.799313	6.813670	-0.038052	3.492131
191.378463	4109.828273	6.818675	-0.038078	3.495377
191.497321	4117.839255	6.823680	-0.038105	3.498613
191.702502	4125.850233	6.828685	-0.038149	3.501849
192.032978	4133.864440	6.833690	-0.038215	3.505087
191.983594	4141.903943	6.838694	-0.038211	3.508321
192.159441	4149.938915	6.843699	-0.038249	3.511557
192.276520	4157.952468	6.848704	-0.038276	3.514779
192.521246	4166.008787	6.853709	-0.038327	3.518019
192.667202	4174.035804	6.858714	-0.038359	3.521242
192.903126	4181.990857	6.863718	-0.038409	3.524435
193.086294	4190.082141	6.868723	-0.038448	3.527679
193.175043	4198.091260	6.873728	-0.038470	3.530883
193.378466	4206.151407	6.878733	-0.038513	3.534109
193.701663	4214.198228	6.883738	-0.038578	3.537330
193.891167	4222.152156	6.888742	-0.038619	3.540507
194.338026	4230.193556	6.893747	-0.038707	3.543723
194.542693	4238.216683	6.898752	-0.038750	3.546923
194.627552	4246.274181	6.903757	-0.038771	3.550129
194.779249	4254.408718	6.908762	-0.038805	3.553365
195.000008	4262.414973	6.913766	-0.038851	3.556549
195.423713	4270.338622	6.918771	-0.038935	3.559703
195.553121	4278.348042	6.923776	-0.038964	3.562880
195.642190	4286.377911	6.928781	-0.038986	3.566061
195.944238	4294.377994	6.933786	-0.039048	3.569234
196.048470	4302.413303	6.938790	-0.039072	3.572412
196.440408	4310.464819	6.943795	-0.039150	3.575602
196.553509	4318.447459	6.948800	-0.039177	3.578753
196.803154	4326.475600	6.953805	-0.039228	3.581924
196.893167	4334.494009	6.958810	-0.039250	3.585083
197.154537	4342.488069	6.963814	-0.039304	3.588235
197.765719	4350.560968	6.968819	-0.039423	3.591425
197.966484	4358.572266	6.973824	-0.039466	3.594577
197.956146	4366.597901	6.978829	-0.039469	3.597725
198.262175	4374.609488	6.983834	-0.039531	3.600874
198.562242	4382.587985	6.988838	-0.039592	3.604007
198.690667	4390.664827	6.993843	-0.039621	3.607171
198.978999	4398.657563	6.998848	-0.039680	3.610303
199.430186	4406.716205	7.003853	-0.039769	3.613463
199.682491	4414.766558	7.008858	-0.039822	3.616612
199.750046	4422.741745	7.013862	-0.039839	3.619723
200.058232	4430.762235	7.018867	-0.039902	3.622856
200.092252	4438.805021	7.023872	-0.039914	3.625988
200.388365	4446.831641	7.028877	-0.039974	3.629117
200.504416	4454.910840	7.033882	-0.040001	3.632259
200.485859	4462.945307	7.038886	-0.040002	3.635378
200.868741	4470.941932	7.043891	-0.040079	3.638490
200.985029	4478.964818	7.048896	-0.040106	3.641602
201.167256	4486.932004	7.053901	-0.040145	3.644692
201.436032	4494.958215	7.058906	-0.040200	3.647804
201.381373	4502.989339	7.063910	-0.040195	3.650907
201.854502	4511.055090	7.068915	-0.040289	3.654035
202.188437	4519.065422	7.073920	-0.040356	3.657135
201.987117	4527.097211	7.078925	-0.040324	3.660226
202.360308	4535.089477	7.083930	-0.040398	3.663315
202.742656	4543.107519	7.088934	-0.040475	3.666411
202.918691	4551.144792	7.093939	-0.040513	3.669506
202.770483	4559.215597	7.098944	-0.040490	3.672604
202.979640	4567.224474	7.103949	-0.040534	3.675684
203.249416	4575.215764	7.108954	-0.040590	3.678756
203.183482	4583.253333	7.113958	-0.040583	3.681835
203.626222	4591.258935	7.118963	-0.040670	3.684912
203.956568	4599.269080	7.123968	-0.040737	3.687986
204.284038	4607.307491	7.128973	-0.040803	3.691067
204.495562	4615.358768	7.133978	-0.040848	3.694148
204.619002	4623.370275	7.138982	-0.040876	3.697209
204.905954	4631.345842	7.143987	-0.040935	3.700257
205.272738	4639.398325	7.148992	-0.041008	3.703335
205.618624	4647.414735	7.153997	-0.041078	3.706395
205.837040	4655.454408	7.159002	-0.041124	3.709459
205.787520	4663.514043	7.164006	-0.041120	3.712521
206.149789	4671.591609	7.169011	-0.041192	3.715597
206.493596	4679.528240	7.174016	-0.041261	3.718617
206.610518	4687.568394	7.179021	-0.041288	3.721668
206.954174	4695.533117	7.184026	-0.041358	3.724694
207.048498	4703.555006	7.189030	-0.041380	3.727732
207.242225	4711.601129	7.194035	-0.041422	3.730780
207.349666	4719.655251	7.199040	-0.041447	3.733826
207.767347	4727.653420	7.204045	-0.041530	3.736856
208.057232	4735.633193	7.209050	-0.041589	3.739874
208.124689	4743.684861	7.214054	-0.041607	3.742910
208.471177	4751.701617	7.219059	-0.041676	3.745938
208.515527	4759.727247	7.224064	-0.041690	3.748960
208.652406	4767.787683	7.229069	-0.041721	3.751994
208.853217	4775.808360	7.234074	-0.041763	3.755012
209.039079	4783.792418	7.239078	-0.041803	3.758014
209.301935	4791.867296	7.244083	-0.041857	3.761049
209.425313	4799.844052	7.249088	-0.041885	3.764042
209.839164	4807.858660	7.254093	-0.041968	3.767053
209.939154	4815.915688	7.259098	-0.041991	3.770071
209.974519	4823.926351	7.264102	-0.042003	3.773067
210.227405	4832.008809	7.269107	-0.042056	3.776092
210.648375	4839.958048	7.274112	-0.042139	3.779069
210.746737	4848.005161	7.279117	-0.042163	3.782073
211.067227	4856.009370	7.284122	-0.042227	3.785064
211.206655	4864.052683	7.289126	-0.042259	3.788063
211.404222	4872.098134	7.294131	-0.042301	3.791061
211.560945	4880.136515	7.299136	-0.042335	3.794053
211.657873	4888.173929	7.304141	-0.042358	3.797042
212.014531	4896.110703	7.309146	-0.042430	3.799996
212.089346	4904.115009	7.314150	-0.042449	3.802967
212.425860	4912.140611	7.319155	-0.042517	3.805949
212.427983	4920.176170	7.324160	-0.042522	3.808925
212.562956	4928.208601	7.329165	-0.042553	3.811901
212.887394	4936.233848	7.334170	-0.042618	3.814876
213.144306	4944.225458	7.339174	-0.042671	3.817834
213.411623	4952.245625	7.344179	-0.042726	3.820801
213.557210	4960.254590	7.349184	-0.042759	3.823759
213.644827	4968.295173	7.354189	-0.042780	3.826725
213.996105	4976.301561	7.359194	-0.042851	3.829681
214.067951	4984.387035	7.364198	-0.042869	3.832659
214.381664	4992.377663	7.369203	-0.042933	3.835604
214.539352	5000.391033	7.374208	-0.042968	3.838552
214.722833	5008.411739	7.379213	-0.043007	3.841501
214.904831	5016.410689	7.384218	-0.043046	3.844440
215.071622	5024.424361	7.389222	-0.043082	3.847381
215.576345	5032.422871	7.394227	-0.043181	3.850322
215.694299	5040.519995	7.399232	-0.043209	3.853288
215.839469	5048.527991	7.404237	-0.043241	3.856221
216.036510	5056.536731	7.409242	-0.043283	3.859152
216.133977	5064.558828	7.414246	-0.043306	3.862084
216.297337	5072.564639	7.419251	-0.043342	3.865009
216.539444	5080.624542	7.424256	-0.043392	3.867953
216.841903	5088.664277	7.429261	-0.043453	3.870888
216.931498	5096.929352	7.434266	-0.043476	3.873900
217.040061	5104.865097	7.439270	-0.043501	3.876789
217.253463	5112.765102	7.444275	-0.043546	3.879665
217.578176	5120.794062	7.449280	-0.043611	3.882588
217.933295	5128.736401	7.454285	-0.043683	3.885478
218.145423	5136.820701	7.459290	-0.043727	3.888415
218.181144	5144.811983	7.464294	-0.043739	3.891312
218.399992	5152.840110	7.469299	-0.043785	3.894224
218.655516	5160.868967	7.474304	-0.043838	3.897135
218.832052	5168.830356	7.479309	-0.043876	3.900017
219.059621	5176.874564	7.484314	-0.043924	3.902929
219.200111	5184.857624	7.489318	-0.043955	3.905814
219.478388	5192.905300	7.494323	-0.044012	3.908723
219.492133	5200.947625	7.499328	-0.044020	3.911623
219.451670	5208.945841	7.504333	-0.044017	3.914504
219.851460	5216.984651	7.509338	-0.044097	3.917406
220.032634	5224.953069	7.514342	-0.044136	3.920276
220.408530	5232.969643	7.519347	-0.044211	3.923164
220.676560	5240.973409	7.524352	-0.044266	3.926045
220.670201	5249.010930	7.529357	-0.044270	3.928930
220.812464	5257.071278	7.534362	-0.044302	3.931823
220.980660	5265.072727	7.539366	-0.044338	3.934694
221.465047	5273.095732	7.544371	-0.044434	3.937577
221.545979	5281.103844	7.549376	-0.044454	3.940444
221.562709	5289.093934	7.554381	-0.044462	3.943302
221.744756	5297.157721	7.559386	-0.044501	3.946187
221.966387	5305.131977	7.564390	-0.044548	3.949039
222.334482	5313.206462	7.569395	-0.044622	3.951927
222.475274	5321.260420	7.574400	-0.044653	3.954801
222.801510	5329.206139	7.579405	-0.044719	3.957638
222.796715	5337.253502	7.584410	-0.044723	3.960503
222.616032	5345.253714	7.589414	-0.044695	3.963347
223.077524	5353.268375	7.594419	-0.044786	3.966204
223.178616	5361.257862	7.599424	-0.044810	3.969045
223.473929	5369.310750	7.604429	-0.044870	3.971909
223.759749	5377.381476	7.609434	-0.044929	3.974777
224.024295	5385.370190	7.614438	-0.044983	3.977614
224.014638	5393.391693	7.619443	-0.044986	3.980455
223.990975	5401.410765	7.624448	-0.044987	3.983294
224.458227	5409.433902	7.629453	-0.045079	3.986140
224.720806	5417.438005	7.634458	-0.045134	3.988974
224.710410	5425.446366	7.639462	-0.045137	3.991803
225.093825	5433.537869	7.644467	-0.045213	3.994665
225.468932	5441.555159	7.649472	-0.045288	3.997499
225.666319	5449.532352	7.654477	-0.045330	4.000314
225.964970	5457.567407	7.659482	-0.045391	4.003150
225.956792	5465.585769	7.664486	-0.045395	4.005972
226.051281	5473.605173	7.669491	-0.045418	4.008794
226.259115	5481.658965	7.674496	-0.045462	4.011628
226.386518	5489.638553	7.679501	-0.045491	4.014433
226.782636	5497.678589	7.684506	-0.045569	4.017261
226.774962	5505.657718	7.689510	-0.045573	4.020060
227.070376	5513.696796	7.694515	-0.045633	4.022882
227.271867	5521.743981	7.699520	-0.045676	4.025704
227.316290	5529.756461	7.704525	-0.045690	4.028509
227.649680	5537.776296	7.709530	-0.045757	4.031319
227.826413	5545.883701	7.714534	-0.045795	4.034155
228.068076	5553.883222	7.719539	-0.045845	4.036953
228.275067	5561.833514	7.724544	-0.045889	4.039731
228.530718	5569.841022	7.729549	-0.045942	4.042528
228.992056	5577.824853	7.734554	-0.046033	4.045317
228.962532	5585.856647	7.739558	-0.046033	4.048114
229.061908	5593.879598	7.744563	-0.046056	4.050908
229.283651	5601.919180	7.749568	-0.046103	4.053708
229.429903	5609.932520	7.754573	-0.046135	4.056495
229.637481	5617.962385	7.759578	-0.046179	4.059287
229.758258	5625.963663	7.764582	-0.046207	4.062066
229.799051	5633.950352	7.769587	-0.046219	4.064837
229.866003	5642.037855	7.774592	-0.046237	4.067641
230.209041	5650.003430	7.779597	-0.046306	4.070405
230.381250	5658.063593	7.784602	-0.046343	4.073197
230.258639	5666.059080	7.789606	-0.046326	4.075961
230.427218	5674.070863	7.794611	-0.046362	4.078733
230.801298	5682.097151	7.799616	-0.046437	4.081510
230.742326	5690.069363	7.804621	-0.046431	4.084261
230.956988	5698.148384	7.809626	-0.046477	4.087051
231.158908	5706.103062	7.814630	-0.046519	4.089796
231.472761	5714.158521	7.819635	-0.046583	4.092575
231.416748	5722.183188	7.824640	-0.046578	4.095337
231.694615	5730.168550	7.829645	-0.046635	4.098088
231.833480	5738.226531	7.834650	-0.046666	4.100860
231.896669	5746.199297	7.839654	-0.046683	4.103600
232.213068	5754.253275	7.844659	-0.046747	4.106369
232.370652	5762.255135	7.849664	-0.046781	4.109116
232.461183	5770.327808	7.854669	-0.046804	4.111885
232.658118	5778.389209	7.859674	-0.046845	4.114650
232.955549	5786.361151	7.864678	-0.046906	4.117383
233.174698	5794.363337	7.869683	-0.046952	4.120124
233.050923	5802.347097	7.874688	-0.046934	4.122852
233.417335	5810.333606	7.879693	-0.047007	4.125586
233.681565	5818.412536	7.884698	-0.047062	4.128348
233.594283	5826.464028	7.889702	-0.047051	4.131094
233.826081	5834.497393	7.894707	-0.047099	4.133837
234.116593	5842.507506	7.899712	-0.047159	4.136570
234.375880	5850.479227	7.904717	-0.047212	4.139288
234.499724	5858.540043	7.909722	-0.047240	4.142033
234.569668	5866.498902	7.914726	-0.047258	4.144741
234.945638	5874.561565	7.919731	-0.047334	4.147485
235.285527	5882.596057	7.924736	-0.047402	4.150218
235.181145	5890.630306	7.929741	-0.047388	4.152944
235.570582	5898.662821	7.934746	-0.047466	4.155673
235.454493	5906.628831	7.939750	-0.047449	4.158372
235.601348	5914.657345	7.944755	-0.047482	4.161094
235.831152	5922.654226	7.949760	-0.047530	4.163804
236.037786	5930.676588	7.954765	-0.047573	4.166520
236.205656	5938.711126	7.959770	-0.047610	4.169239
236.137581	5946.754260	7.964774	-0.047602	4.171955
236.470508	5954.764298	7.969779	-0.047670	4.174664
236.486067	5962.819799	7.974784	-0.047678	4.177382
236.662442	5970.737277	7.979789	-0.047716	4.180054
237.159840	5978.807876	7.984794	-0.047813	4.182779
237.157576	5986.790762	7.989798	-0.047818	4.185467
237.339956	5994.826643	7.994803	-0.047857	4.188174
237.548875	6002.862310	7.999808	-0.047902	4.190879
237.786058	6010.959038	8.004813	-0.047951	4.193603
237.917123	6019.000347	8.009818	-0.047981	4.196305
238.232017	6026.915507	8.014822	-0.048044	4.198965
238.515901	6034.887996	8.019827	-0.048102	4.201643
238.540297	6042.881225	8.024832	-0.048112	4.204323
238.569778	6050.918564	8.029837	-0.048123	4.207016
238.848306	6058.939425	8.034842	-0.048180	4.209704
238.974390	6067.003792	8.039846	-0.048209	4.212404
239.107917	6074.977902	8.044851	-0.048239	4.215071
239.352679	6083.057506	8.049856	-0.048289	4.217774
239.518357	6091.007301	8.054861	-0.048325	4.220430
239.681669	6099.056761	8.059866	-0.048361	4.223118
239.705227	6107.005067	8.064870	-0.048371	4.225770
239.991752	6115.038727	8.069875	-0.048429	4.228450
240.083829	6123.103912	8.074880	-0.048451	4.231138
240.198378	6131.118267	8.079885	-0.048478	4.233807
240.574672	6139.208112	8.084890	-0.048553	4.236501
240.720238	6147.110727	8.089894	-0.048585	4.239130
240.753545	6155.192570	8.094899	-0.048597	4.241816
241.034612	6163.161583	8.099904	-0.048654	4.244464
241.148321	6171.221322	8.104909	-0.048681	4.247140
241.398310	6179.252269	8.109914	-0.048733	4.249806
241.384579	6187.270212	8.114918	-0.048735	4.252463
241.760519	6195.304168	8.119923	-0.048810	4.255127
241.973327	6203.351538	8.124928	-0.048855	4.257793
241.944619	6211.262352	8.129933	-0.048855	4.260409
242.145994	6219.320162	8.134938	-0.048898	4.263075
242.261157	6227.308835	8.139942	-0.048924	4.265715
242.460706	6235.364598	8.144947	-0.048967	4.268377
242.877697	6243.391373	8.149952	-0.049050	4.271029
242.852862	6251.490709	8.154957	-0.049050	4.273699
243.137148	6259.505611	8.159962	-0.049108	4.276343
243.005842	6267.440496	8.164966	-0.049089	4.278955
243.415349	6275.434715	8.169971	-0.049170	4.281590
243.424316	6283.449859	8.174976	-0.049177	4.284226
243.574081	6291.462617	8.179981	-0.049210	4.286862
243.825904	6299.531066	8.184986	-0.049263	4.289514
243.737232	6307.537888	8.189990	-0.049251	4.292142
243.859490	6315.565357	8.194995	-0.049279	4.294777
244.122928	6323.601047	8.200000	-0.049333	4.297415
244.237939	6331.543402	8.205005	-0.049360	4.300018
244.571346	6339.588379	8.210010	-0.049427	4.302656
244.741878	6347.573603	8.215014	-0.049464	4.305271
244.873600	6355.599042	8.220019	-0.049494	4.307897
245.241650	6363.671687	8.225024	-0.049568	4.310539
244.973399	6371.698215	8.230029	-0.049523	4.313159
245.176296	6379.770357	8.235034	-0.049566	4.315796
245.349145	6387.699866	8.240038	-0.049603	4.318385
245.558918	6395.686047	8.245043	-0.049648	4.320991
245.861337	6403.737351	8.250048	-0.049709	4.323617
245.870846	6411.739772	8.255053	-0.049716	4.326224
246.205400	6419.771544	8.260058	-0.049784	4.328841
246.306439	6427.783648	8.265062	-0.049808	4.331448
246.576184	6435.798905	8.270067	-0.049863	4.334056
246.821544	6443.864802	8.275072	-0.049914	4.336678
246.942798	6451.804639	8.280077	-0.049942	4.339257
247.332463	6459.854281	8.285082	-0.050019	4.341872
247.475440	6467.808157	8.290086	-0.050051	4.344453
247.463470	6475.876966	8.295091	-0.050054	4.347068
247.544680	6483.887999	8.300096	-0.050074	4.349664
247.808967	6491.898224	8.305101	-0.050129	4.352259
248.084453	6500.069486	8.310106	-0.050185	4.354904
248.028591	6508.013854	8.315110	-0.050180	4.357473
248.234869	6515.943249	8.320115	-0.050224	4.360037
248.525121	6524.005339	8.325120	-0.050283	4.362642
248.316966	6531.972639	8.330125	-0.050249	4.365213
248.747609	6540.043714	8.335130	-0.050335	4.367819
248.713434	6548.004568	8.340134	-0.050334	4.370385
248.932226	6556.026434	8.345139	-0.050380	4.372971
248.893174	6564.100581	8.350144	-0.050378	4.375571
249.098165	6572.076078	8.355149	-0.050421	4.378139
249.438750	6580.053894	8.360154	-0.050489	4.380706
249.485131	6588.098150	8.365158	-0.050503	4.383292
249.621075	6596.107683	8.370163	-0.050534	4.385866
249.828522	6604.137267	8.375168	-0.050578	4.388445
249.978906	6612.092844	8.380173	-0.050611	4.390999
250.125529	6620.209975	8.385178	-0.050643	4.393603
250.125657	6628.242868	8.390182	-0.050649	4.396177
250.188004	6636.209236	8.395187	-0.050665	4.398729
250.340586	6644.225599	8.400192	-0.050699	4.401296
250.332713	6652.201500	8.405197	-0.050703	4.403847
250.976759	6660.275040	8.410202	-0.050828	4.406432
251.035578	6668.238801	8.415206	-0.050844	4.408977
251.348323	6676.303915	8.420211	-0.050907	4.411554
251.454865	6684.360452	8.425216	-0.050932	4.414126
251.436763	6692.324771	8.430221	-0.050934	4.416667
251.590305	6700.381194	8.435226	-0.050968	4.419236
251.936164	6708.409111	8.440230	-0.051038	4.421795
251.982969	6716.369745	8.445235	-0.051052	4.424330
252.057889	6724.418953	8.450240	-0.051071	4.426892
252.092862	6732.406668	8.455245	-0.051082	4.429433
252.548512	6740.496177	8.460250	-0.051172	4.432006
252.692578	6748.542839	8.465254	-0.051204	4.434563
252.703068	6756.564578	8.470259	-0.051212	4.437110
252.714455	6764.494478	8.475264	-0.051219	4.439626
252.769213	6772.503146	8.480269	-0.051234	4.442167
253.088834	6780.505043	8.485274	-0.051299	4.444704
253.253782	6788.536336	8.490278	-0.051335	4.447249
253.276812	6796.545518	8.495283	-0.051344	4.449785
253.338143	6804.607163	8.500288	-0.051361	4.452336
253.572042	6812.594287	8.505293	-0.051410	4.454862
254.159793	6820.643965	8.510298	-0.051524	4.457408
254.183951	6828.600475	8.515302	-0.051534	4.459922
254.351386	6836.632008	8.520307	-0.051570	4.462458
254.413625	6844.636746	8.525312	-0.051587	4.464983
254.520145	6852.669310	8.530317	-0.051612	4.467517
254.680289	6860.710833	8.535322	-0.051647	4.470051
254.741292	6868.724379	8.540326	-0.051664	4.472575
254.923204	6876.744143	8.545331	-0.051703	4.475101
255.149190	6884.769038	8.550336	-0.051750	4.477626
255.172779	6892.693417	8.555341	-0.051760	4.480118
255.278068	6900.793306	8.560346	-0.051785	4.482663
255.502765	6908.737547	8.565351	-0.051832	4.485159
255.648940	6916.810454	8.570355	-0.051864	4.487693
255.873264	6924.823522	8.575360	-0.051911	4.490208
256.075052	6932.868285	8.580365	-0.051954	4.492731
256.168070	6940.858876	8.585370	-0.051976	4.495235
256.374067	6948.883847	8.590375	-0.052020	4.497749
256.492360	6956.816403	8.595379	-0.052047	4.500232
256.550727	6964.901663	8.600384	-0.052063	4.502762
256.759362	6972.891332	8.605389	-0.052107	4.505260
256.883730	6980.952189	8.610394	-0.052135	4.507779
256.865965	6988.947774	8.615399	-0.052137	4.510276
256.895341	6997.007447	8.620403	-0.052148	4.512792
257.191975	7005.042531	8.625408	-0.052208	4.515299
257.378775	7013.042972	8.630413	-0.052248	4.517794
257.495087	7020.995320	8.635418	-0.052275	4.520272
257.787842	7029.038057	8.640423	-0.052335	4.522778
258.124091	7036.974708	8.645427	-0.052403	4.525249
258.125917	7045.061662	8.650432	-0.052408	4.527764
258.272875	7053.015561	8.655437	-0.052441	4.530238
258.449605	7061.101315	8.660442	-0.052479	4.532751
258.539522	7069.094634	8.665447	-0.052501	4.535233
258.771992	7077.093531	8.670451	-0.052549	4.537716
259.008150	7085.131113	8.675456	-0.052599	4.540210
259.171827	7093.121247	8.680461	-0.052634	4.542688
259.223671	7101.146655	8.685466	-0.052649	4.545175
259.234456	7109.188802	8.690471	-0.052656	4.547666
259.668380	7117.175731	8.695475	-0.052742	4.550139
259.883363	7125.237895	8.700480	-0.052788	4.552633
259.894484	7133.206540	8.705485	-0.052795	4.555097
260.157238	7141.280457	8.710490	-0.052849	4.557592
260.298406	7149.226972	8.715495	-0.052880	4.560047
260.403290	7157.278133	8.720499	-0.052905	4.562532
260.666532	7165.287570	8.725504	-0.052959	4.565004
260.781747	7173.283773	8.730509	-0.052986	4.567469
261.095565	7181.296831	8.735514	-0.053050	4.569939
261.242618	7189.343291	8.740519	-0.053082	4.572418
261.390843	7197.354616	8.745523	-0.053115	4.574884
261.742229	7205.427596	8.750528	-0.053186	4.577368
261.949360	7213.375508	8.755533	-0.053229	4.579813
262.092273	7221.444764	8.760538	-0.053261	4.582293
262.186331	7229.407755	8.765543	-0.053284	4.584739
262.217032	7237.470792	8.770547	-0.053295	4.587214
262.436455	7245.469653	8.775552	-0.053341	4.589669
262.688449	7253.473852	8.780557	-0.053393	4.592124
262.875895	7261.551820	8.785562	-0.053433	4.594600
262.917516	7269.571218	8.790567	-0.053446	4.597056
263.179753	7277.493705	8.795571	-0.053500	4.599482
263.463932	7285.621499	8.800576	-0.053558	4.601969
263.384324	7293.471253	8.805581	-0.053548	4.604370
263.614086	7301.592562	8.810586	-0.053596	4.606853
263.806368	7309.576286	8.815591	-0.053637	4.609292
263.961415	7317.569441	8.820595	-0.053671	4.611733
264.235381	7325.666155	8.825600	-0.053728	4.614204
264.613068	7333.664970	8.830605	-0.053803	4.616644
264.871783	7341.657877	8.835610	-0.053857	4.619080
264.929067	7349.663189	8.840615	-0.053872	4.621520
265.134685	7357.631862	8.845619	-0.053916	4.623946
265.335506	7365.698168	8.850624	-0.053959	4.626402
265.295098	7373.740839	8.855629	-0.053956	4.628848
265.550704	7381.746061	8.860634	-0.054009	4.631282
265.633662	7389.766630	8.865639	-0.054030	4.633720
265.651659	7397.784149	8.870643	-0.054038	4.636155
265.757375	7405.799899	8.875648	-0.054063	4.638588
265.968223	7413.793376	8.880653	-0.054107	4.641013
266.232275	7421.780951	8.885658	-0.054162	4.643435
266.348983	7429.784793	8.890663	-0.054189	4.645861
266.762379	7437.813275	8.895667	-0.054271	4.648293
266.989413	7445.875492	8.900672	-0.054318	4.650734
266.937259	7453.860667	8.905677	-0.054314	4.653150
266.999933	7461.890632	8.910682	-0.054331	4.655579
267.366147	7469.911434	8.915687	-0.054404	4.658003
267.429184	7477.882718	8.920691	-0.054421	4.660411
267.533464	7485.926572	8.925696	-0.054446	4.662840
267.707177	7493.878731	8.930701	-0.054483	4.665240
268.071487	7501.957001	8.935706	-0.054556	4.667676
267.839676	7509.984128	8.940711	-0.054518	4.670097
267.919878	7518.013697	8.945715	-0.054538	4.672516
268.345396	7526.096855	8.950720	-0.054623	4.674950
268.413296	7534.130706	8.955725	-0.054641	4.677369
268.430087	7542.013828	8.960730	-0.054649	4.679740
268.611377	7550.038940	8.965735	-0.054688	4.682153
268.922025	7557.992119	8.970739	-0.054751	4.684543
268.807408	7566.091484	8.975744	-0.054735	4.686977
268.912679	7574.024744	8.980749	-0.054760	4.689358
269.123721	7582.119879	8.985754	-0.054804	4.691787
269.144985	7590.154564	8.990759	-0.054813	4.694197
269.483635	7598.146545	8.995763	-0.054882	4.696592
269.735858	7606.100463	9.000768	-0.054934	4.698975
269.681207	7614.155425	9.005773	-0.054929	4.701387
269.864670	7622.121293	9.010778	-0.054968	4.703771
270.170768	7630.176743	9.015783	-0.055030	4.706181
270.107127	7638.173053	9.020787	-0.055024	4.708572
270.392418	7646.245104	9.025792	-0.055082	4.710983
270.506880	7654.246859	9.030797	-0.055108	4.713373
270.760139	7662.323948	9.035802	-0.055161	4.715784
270.811478	7670.298925	9.040807	-0.055176	4.718164
270.761787	7678.246723	9.045811	-0.055171	4.720534
271.254689	7686.314321	9.050816	-0.055268	4.722938
271.292218	7694.267886	9.055821	-0.055281	4.725308
271.292496	7702.347817	9.060826	-0.055286	4.727714
271.479511	7710.384311	9.065831	-0.055326	4.730105
271.702638	7718.372812	9.070835	-0.055373	4.732481
271.864587	7726.422587	9.075840	-0.055408	4.734874
271.832056	7734.445144	9.080845	-0.055407	4.737258
271.998076	7742.364418	9.085850	-0.055443	4.739610
272.152077	7750.469543	9.090855	-0.055477	4.742016
272.272688	7758.398540	9.095859	-0.055505	4.744368
272.486114	7766.478878	9.100864	-0.055550	4.746764
272.580683	7774.475705	9.105869	-0.055572	4.749134
272.721248	7782.482354	9.110874	-0.055604	4.751506
272.980977	7790.574558	9.115879	-0.055657	4.753902
273.321385	7798.543165	9.120883	-0.055726	4.756259
273.346538	7806.567060	9.125888	-0.055736	4.758633
273.336997	7814.533310	9.130893	-0.055739	4.760988
273.643453	7822.561224	9.135898	-0.055802	4.763360
273.601458	7830.593206	9.140903	-0.055799	4.765732
273.727187	7838.579452	9.145907	-0.055827	4.768090
274.053345	7846.607171	9.150912	-0.055893	4.770458
274.075708	7854.664741	9.155917	-0.055903	4.772834
274.315922	7862.659281	9.160922	-0.055953	4.775190
274.435222	7870.693357	9.165927	-0.055980	4.777557
274.664450	7878.622675	9.170931	-0.056028	4.779891
274.849097	7886.721912	9.175936	-0.056068	4.782274
274.931735	7894.624310	9.180941	-0.056088	4.784599
275.257425	7902.718781	9.185946	-0.056154	4.786978
275.162757	7910.687114	9.190951	-0.056142	4.789320
275.180340	7918.755546	9.195955	-0.056150	4.791691
275.612368	7926.842564	9.200960	-0.056236	4.794063
275.722760	7934.809817	9.205965	-0.056261	4.796401
275.843881	7942.787555	9.210970	-0.056289	4.798741
275.871830	7950.798710	9.215975	-0.056300	4.801089
276.241185	7958.767920	9.220979	-0.056373	4.803423
276.209414	7966.805257	9.225984	-0.056373	4.805777
276.256220	7974.847773	9.230989	-0.056387	4.808132
276.361151	7982.840760	9.235994	-0.056411	4.810470
276.717061	7990.392245	9.240999	-0.056483	4.812677
276.773820	7995.052175	9.246003	-0.056496	4.814039
277.088882	7997.642087	9.251008	-0.056556	4.814795
277.061188	7999.005746	9.256013	-0.056552	4.815193
277.056745	7999.474644	9.261018	-0.056552	4.815331
277.254229	8000.612454	9.266023	-0.056589	4.815662
277.303533	8000.575869	9.271027	-0.056598	4.815651
277.405924	8000.619216	9.276032	-0.056617	4.815663
277.544675	8000.506110	9.281037	-0.056643	4.815630
277.614090	8000.531821	9.286042	-0.056656	4.815637
277.667560	8000.607484	9.291047	-0.056666	4.815659
277.707819	8000.595322	9.296051	-0.056673	4.815655
277.790565	8000.592407	9.301056	-0.056689	4.815654
277.921925	8000.614863	9.306061	-0.056713	4.815660
277.805590	8000.477263	9.311066	-0.056691	4.815620
277.830116	8000.618690	9.316071	-0.056696	4.815661
277.922031	8000.526181	9.321075	-0.056713	4.815634
278.038822	8000.504594	9.326080	-0.056735	4.815627
277.989046	8000.609543	9.331085	-0.056726	4.815658
278.231993	8000.562253	9.336090	-0.056771	4.815643
278.180394	8000.536829	9.341095	-0.056761	4.815636
278.099890	8000.581443	9.346099	-0.056746	4.815649
278.222488	8000.517216	9.351104	-0.056769	4.815630
278.232232	8000.563315	9.356109	-0.056771	4.815643
278.341527	8000.617461	9.361114	-0.056791	4.815658
278.213856	8000.522409	9.366119	-0.056767	4.815631
278.431030	8000.623201	9.371123	-0.056808	4.815660
278.532716	8000.500937	9.376128	-0.056826	4.815623
278.536075	8000.597145	9.381133	-0.056827	4.815651
278.559549	8000.619965	9.386138	-0.056831	4.815658
278.649020	8000.484679	9.391143	-0.056848	4.815618
278.558736	8000.516312	9.396147	-0.056831	4.815628
278.617684	8000.568562	9.401152	-0.056842	4.815643
278.489071	8000.555760	9.406157	-0.056818	4.815640
278.523053	8000.532811	9.411162	-0.056824	4.815633
278.656895	8000.527531	9.416167	-0.056849	4.815631
278.727523	8000.610957	9.421171	-0.056863	4.815655
278.695804	8000.542055	9.426176	-0.056857	4.815635
278.523663	8000.607599	9.431181	-0.056824	4.815655
278.571245	8000.531454	9.436186	-0.056833	4.815632
278.793201	8000.545786	9.441191	-0.056875	4.815635
278.694276	8000.516378	9.446195	-0.056856	4.815627
278.951856	8000.547322	9.451200	-0.056904	4.815635
278.957472	8000.620063	9.456205	-0.056905	4.815656
278.802770	8000.493581	9.461210	-0.056876	4.815620
278.905576	8000.635231	9.466215	-0.056895	4.815661
278.808780	8000.521453	9.471219	-0.056877	4.815628
279.046604	8000.538183	9.476224	-0.056922	4.815632
278.968547	8000.624506	9.481229	-0.056907	4.815657
278.929724	8000.481766	9.486234	-0.056900	4.815616
279.064254	8000.549149	9.491239	-0.056925	4.815635
279.100310	8000.480293	9.496243	-0.056931	4.815615
279.071551	8000.538580	9.501248	-0.056926	4.815632
279.096923	8000.618058	9.506253	-0.056931	4.815655
279.020913	8000.553768	9.511258	-0.056917	4.815636
279.083573	8000.548386	9.516263	-0.056928	4.815635
279.150695	8000.563377	9.521267	-0.056941	4.815639
279.251109	8000.497716	9.526272	-0.056959	4.815619
279.119027	8000.630161	9.531277	-0.056935	4.815658
279.069292	8000.588740	9.536282	-0.056925	4.815646
279.161959	8000.543252	9.541287	-0.056943	4.815633
279.048393	8000.512534	9.546291	-0.056921	4.815624
279.201097	8000.627227	9.551296	-0.056950	4.815657
279.201375	8000.548166	9.556301	-0.056950	4.815634
279.460295	8000.495796	9.561306	-0.056998	4.815617
279.417308	8000.637187	9.566311	-0.056990	4.815659
279.252157	8000.516941	9.571315	-0.056959	4.815625
279.139464	8000.536453	9.576320	-0.056938	4.815631
279.276647	8000.624180	9.581325	-0.056964	4.815656
279.241440	8000.481499	9.586330	-0.056957	4.815614
279.190204	8000.531938	9.591335	-0.056948	4.815629
279.304016	8000.620349	9.596339	-0.056969	4.815655
279.187726	8000.552191	9.601344	-0.056947	4.815635
279.183862	8000.616230	9.606349	-0.056946	4.815654
279.455068	8000.511711	9.611354	-0.056997	4.815622
279.394518	8000.543833	9.616359	-0.056986	4.815632
279.387652	8000.567223	9.621363	-0.056984	4.815639
279.708449	8000.545787	9.626368	-0.057044	4.815631
279.484891	8000.541038	9.631373	-0.057002	4.815631
279.401459	8000.538594	9.636378	-0.056987	4.815630
279.541319	8000.632777	9.641383	-0.057013	4.815657
279.386141	8000.507353	9.646387	-0.056984	4.815621
279.428964	8000.556134	9.651392	-0.056992	4.815635
279.441173	8000.616164	9.656397	-0.056994	4.815653
279.433327	8000.545516	9.661402	-0.056992	4.815632
279.724188	8000.521451	9.666407	-0.057047	4.815624
279.563906	8000.626723	9.671411	-0.057017	4.815655
279.746571	8000.549594	9.676416	-0.057051	4.815632
279.633353	8000.501786	9.681421	-0.057030	4.815618
279.700119	8000.423819	9.686426	-0.057042	4.815595
279.672779	8000.496019	9.691431	-0.057037	4.815616
279.555449	8000.597723	9.696435	-0.057015	4.815647
279.634906	8000.441969	9.701440	-0.057030	4.815601
279.631858	8000.549827	9.706445	-0.057029	4.815632
279.544777	8000.504587	9.711450	-0.057013	4.815620
279.592106	8000.643190	9.716455	-0.057022	4.815660
279.665278	8000.516180	9.721459	-0.057035	4.815622
279.504315	8000.479340	9.726464	-0.057005	4.815612
279.609980	8000.605013	9.731469	-0.057025	4.815649
279.594743	8000.468001	9.736474	-0.057022	4.815609
279.604531	8000.620944	9.741479	-0.057024	4.815653
279.634109	8000.584033	9.746483	-0.057029	4.815642
279.765966	8000.501794	9.751488	-0.057054	4.815618
279.498768	8000.577527	9.756493	-0.057004	4.815641
279.790569	8000.584463	9.761498	-0.057058	4.815642
279.908232	8000.553275	9.766503	-0.057080	4.815632
279.711588	8000.500889	9.771507	-0.057044	4.815618
279.719857	8000.534144	9.776512	-0.057045	4.815627
279.695556	8000.606395	9.781517	-0.057041	4.815649
279.774859	8000.494443	9.786522	-0.057055	4.815616
279.927244	8000.550369	9.791527	-0.057084	4.815631
279.862929	8000.625167	9.796531	-0.057072	4.815653
279.913250	8000.440086	9.801536	-0.057081	4.815599
279.637946	8000.526370	9.806541	-0.057030	4.815626
279.596475	8000.638938	9.811546	-0.057022	4.815659
279.904105	8000.531812	9.816551	-0.057079	4.815626
279.872151	8000.515257	9.821555	-0.057073	4.815621
279.963905	8000.565912	9.826560	-0.057090	4.815636
279.982727	8000.607889	9.831565	-0.057094	4.815648
280.024875	8000.467546	9.836570	-0.057102	4.815606
279.811949	8000.523872	9.841575	-0.057062	4.815624
279.917165	8000.650608	9.846579	-0.057082	4.815660
279.916055	8000.511690	9.851584	-0.057081	4.815620
279.718915	8000.616356	9.856589	-0.057045	4.815651
279.842071	8000.467731	9.861594	-0.057067	4.815607
280.010200	8000.531395	9.866599	-0.057099	4.815625
279.734233	8000.515099	9.871603	-0.057047	4.815622
279.758800	8000.540074	9.876608	-0.057052	4.815629
279.961262	8000.555156	9.881613	-0.057089	4.815632
279.792040	8000.520316	9.886618	-0.057058	4.815623
279.744056	8000.427639	9.891623	-0.057049	4.815596
279.959681	8000.611749	9.896627	-0.057089	4.815649
280.085577	8000.608476	9.901632	-0.057113	4.815647
280.001793	8000.541920	9.906637	-0.057097	4.815628
279.968682	8000.459103	9.911642	-0.057091	4.815604
279.998006	8000.599548	9.916647	-0.057096	4.815645
279.936063	8000.550447	9.921651	-0.057085	4.815631
279.931780	8000.502294	9.926656	-0.057084	4.815617
279.964490	8000.595783	9.931661	-0.057090	4.815644
280.131223	8000.497023	9.936666	-0.057121	4.815615
280.029839	8000.526337	9.941671	-0.057102	4.815624
279.879932	8000.661696	9.946675	-0.057074	4.815664
280.076035	8000.517476	9.951680	-0.057110	4.815621
279.758419	8000.491947	9.956685	-0.057051	4.815615
280.023357	8000.509125	9.961690	-0.057101	4.815619
280.035589	8000.532829	9.966695	-0.057103	4.815626
279.917735	8000.627046	9.971699	-0.057081	4.815654
280.054004	8000.519237	9.976704	-0.057106	4.815621
279.984641	8000.509546	9.981709	-0.057093	4.815619
280.284098	8000.469596	9.986714	-0.057149	4.815606
280.058561	8000.641106	9.991719	-0.057107	4.815657
280.022343	8000.510158	9.996723	-0.057100	4.815619
280.226803	8000.508178	10.001728	-0.057138	4.815617
280.013863	8000.621131	10.006733	-0.057099	4.815651
280.028568	8000.611754	10.011738	-0.057101	4.815649
280.014202	8000.427745	10.016743	-0.057098	4.815595
279.945337	8000.575121	10.021747	-0.057086	4.815638
279.986501	8000.476431	10.026752	-0.057093	4.815609
280.049177	8000.631315	10.031757	-0.057105	4.815654
279.992559	8000.505374	10.036762	-0.057094	4.815618
280.200261	8000.557937	10.041767	-0.057133	4.815632
280.182388	8000.492465	10.046771	-0.057130	4.815613
280.165721	8000.501804	10.051776	-0.057127	4.815616
280.092309	8000.638422	10.056781	-0.057113	4.815656
280.085982	8000.463092	10.061786	-0.057112	4.815605
280.224707	8000.604269	10.066791	-0.057137	4.815646
280.239102	8000.496591	10.071795	-0.057140	4.815614
280.205059	8000.619967	10.076800	-0.057134	4.815650
280.460704	8000.507711	10.081805	-0.057181	4.815616
280.419524	8000.521989	10.086810	-0.057174	4.815621
280.259991	8000.637959	10.091815	-0.057144	4.815655
280.234810	8000.520013	10.096819	-0.057139	4.815621
280.356503	8000.512397	10.101824	-0.057162	4.815618
280.177760	8000.488084	10.106829	-0.057128	4.815612
280.227682	8000.507066	10.111834	-0.057138	4.815617
280.275751	8000.553798	10.116839	-0.057147	4.815631
280.013291	8000.600761	10.121843	-0.057098	4.815646
280.098638	8000.438692	10.126848	-0.057114	4.815598
280.152826	8000.518645	10.131853	-0.057124	4.815621
280.316902	8000.527753	10.136858	-0.057154	4.815623
280.234421	8000.440919	10.141863	-0.057139	4.815598
280.218154	8000.567792	10.146867	-0.057136	4.815635
280.172510	8000.495453	10.151872	-0.057127	4.815614
280.093098	8000.624493	10.156877	-0.057112	4.815652
280.067434	8000.472350	10.161882	-0.057108	4.815608
280.340676	8000.631768	10.166887	-0.057158	4.815653
280.232429	8000.593657	10.171891	-0.057138	4.815642
280.190946	8000.455143	10.176896	-0.057130	4.815602
280.284384	8000.541085	10.181901	-0.057148	4.815627
280.211821	8000.539888	10.186906	-0.057134	4.815627
280.351616	8000.525091	10.191911	-0.057160	4.815622
280.225611	8000.612764	10.196915	-0.057137	4.815648
280.345366	8000.477971	10.201920	-0.057159	4.815608
280.365906	8000.515702	10.206925	-0.057163	4.815619
280.228299	8000.527325	10.211930	-0.057137	4.815623
280.277465	8000.410603	10.216935	-0.057146	4.815589
280.402081	8000.555822	10.221939	-0.057170	4.815631
280.462609	8000.620922	10.226944	-0.057181	4.815649
280.575623	8000.443281	10.231949	-0.057202	4.815597
280.517041	8000.489326	10.236954	-0.057191	4.815611
280.385067	8000.486083	10.241959	-0.057166	4.815610
280.505522	8000.510500	10.246963	-0.057189	4.815617
280.468889	8000.535537	10.251968	-0.057182	4.815624
280.483516	8000.458847	10.256973	-0.057184	4.815602
280.349671	8000.541049	10.261978	-0.057160	4.815626
280.447072	8000.557607	10.266983	-0.057178	4.815631
280.425278	8000.497413	10.271987	-0.057174	4.815613
280.370270	8000.532832	10.276992	-0.057163	4.815624
280.281218	8000.609360	10.281997	-0.057147	4.815647
280.479481	8000.476928	10.287002	-0.057184	4.815607
280.473188	8000.538792	10.292007	-0.057182	4.815625
280.221442	8000.608369	10.297011	-0.057136	4.815647
280.370054	8000.477257	10.302016	-0.057163	4.815608
280.654430	8000.621901	10.307021	-0.057216	4.815649
280.506981	8000.533996	10.312026	-0.057189	4.815624
280.702632	8000.548966	10.317031	-0.057225	4.815627
280.467685	8000.541891	10.322035	-0.057181	4.815626
280.506320	8000.537182	10.327040	-0.057188	4.815625
280.547117	8000.505798	10.332045	-0.057196	4.815615
280.652902	8000.649640	10.337050	-0.057216	4.815657
280.648903	8000.490372	10.342055	-0.057215	4.815610
280.555288	8000.627727	10.347059	-0.057197	4.815651
280.651885	8000.492553	10.352064	-0.057215	4.815611
280.826649	8000.524275	10.357069	-0.057248	4.815619
280.645878	8000.495654	10.362074	-0.057214	4.815612
280.667204	8000.525919	10.367079	-0.057218	4.815621
280.585677	8000.540602	10.372083	-0.057203	4.815625
280.436087	8000.495399	10.377088	-0.057175	4.815613
280.440067	8000.489051	10.382093	-0.057176	4.815611
280.441749	8000.525404	10.387098	-0.057176	4.815621
280.551138	8000.500490	10.392103	-0.057196	4.815614
280.434654	8000.629989	10.397107	-0.057175	4.815652
280.717292	8000.440181	10.402112	-0.057227	4.815595
280.722841	8000.562073	10.407117	-0.057228	4.815631
280.480016	8000.515336	10.412122	-0.057183	4.815618
280.644863	8000.431502	10.417127	-0.057214	4.815593
280.678393	8000.552786	10.422131	-0.057220	4.815628
280.511180	8000.475240	10.427136	-0.057189	4.815606
280.400909	8000.506544	10.432141	-0.057168	4.815616
280.425824	8000.626618	10.437146	-0.057173	4.815651
280.636125	8000.430277	10.442151	-0.057212	4.815593
280.571197	8000.620458	10.447155	-0.057200	4.815649
280.637615	8000.507224	10.452160	-0.057212	4.815615
280.483905	8000.501487	10.457165	-0.057183	4.815614
280.471912	8000.575009	10.462170	-0.057181	4.815636
280.433857	8000.527369	10.467175	-0.057174	4.815622
280.343944	8000.513065	10.472179	-0.057157	4.815618
280.634592	8000.549899	10.477184	-0.057211	4.815628
280.501218	8000.534880	10.482189	-0.057186	4.815624
280.543512	8000.480015	10.487194	-0.057194	4.815608
280.799573	8000.540854	10.492199	-0.057242	4.815624
280.703159	8000.527512	10.497203	-0.057224	4.815621
280.722060	8000.539573	10.502208	-0.057227	4.815624
280.840019	8000.536170	10.507213	-0.057249	4.815623
280.557989	8000.515498	10.512218	-0.057197	4.815618
280.705232	8000.566000	10.517223	-0.057224	4.815632
280.687128	8000.566767	10.522227	-0.057221	4.815632
280.777081	8000.435758	10.527232	-0.057237	4.815594
280.732066	8000.468136	10.532237	-0.057229	4.815603
280.910225	8000.473203	10.537242	-0.057262	4.815604
280.857881	8000.398615	10.542247	-0.057252	4.815582
280.726727	8000.595186	10.547251	-0.057228	4.815641
280.805132	8000.462917	10.552256	-0.057243	4.815601
280.843449	8000.608855	10.557261	-0.057250	4.815644
280.607765	8000.595357	10.562266	-0.057206	4.815641
280.732268	8000.398672	10.567271	-0.057229	4.815583
280.718570	8000.607860	10.572275	-0.057226	4.815644
280.688018	8000.437471	10.577280	-0.057221	4.815595
280.805760	8000.623180	10.582285	-0.057243	4.815648
280.603181	8000.485218	10.587290	-0.057205	4.815609
280.929760	8000.533329	10.592295	-0.057266	4.815621
280.580588	8000.601302	10.597299	-0.057201	4.815643
280.642796	8000.560654	10.602304	-0.057212	4.815631
280.782512	8000.523418	10.607309	-0.057238	4.815619
280.671324	8000.539749	10.612314	-0.057217	4.815625
280.725081	8000.548110	10.617319	-0.057227	4.815627
280.772686	8000.600177	10.622323	-0.057236	4.815642
280.714699	8000.491306	10.627328	-0.057225	4.815610
280.693107	8000.508043	10.632333	-0.057221	4.815615
280.710036	8000.589522	10.637338	-0.057224	4.815639
280.779096	8000.552192	10.642343	-0.057237	4.815628
280.704968	8000.511436	10.647347	-0.057223	4.815616
280.627940	8000.603121	10.652352	-0.057209	4.815643
280.769872	8000.524252	10.657357	-0.057235	4.815620
280.806733	8000.599648	10.662362	-0.057242	4.815641
280.724278	8000.318355	10.667367	-0.057227	4.815560
280.696058	8000.499524	10.672371	-0.057222	4.815613
280.719499	8000.517002	10.677376	-0.057226	4.815618
280.508777	8000.579775	10.682381	-0.057187	4.815637
280.622668	8000.585921	10.687386	-0.057208	4.815638
280.748911	8000.468330	10.692391	-0.057231	4.815603
280.593869	8000.566209	10.697395	-0.057202	4.815633
280.637728	8000.640652	10.702400	-0.057211	4.815654
280.768347	8000.553049	10.707405	-0.057235	4.815628
280.818183	8000.476938	10.712410	-0.057244	4.815606
280.732289	8000.541766	10.717415	-0.057228	4.815625
280.688201	8000.518600	10.722419	-0.057220	4.815618
280.984983	8000.442280	10.727424	-0.057275	4.815595
280.932273	8000.532228	10.732429	-0.057265	4.815621
280.826035	8000.571078	10.737434	-0.057245	4.815633
281.085082	8000.519780	10.742439	-0.057294	4.815617
280.890038	8000.624481	10.747443	-0.057257	4.815648
280.878961	8000.466165	10.752448	-0.057255	4.815602
280.910949	8000.496605	10.757453	-0.057261	4.815611
280.814715	8000.521730	10.762458	-0.057243	4.815619
280.890647	8000.579605	10.767463	-0.057257	4.815635
280.764690	8000.630952	10.772467	-0.057234	4.815651
280.834117	8000.391691	10.777472	-0.057247	4.815581
280.634989	8000.614922	10.782477	-0.057210	4.815647
280.563627	8000.577417	10.787482	-0.057196	4.815636
280.652627	8000.546826	10.792487	-0.057213	4.815627
280.693140	8000.544285	10.797491	-0.057220	4.815626
280.727740	8000.502114	10.802496	-0.057227	4.815613
280.850006	8000.518014	10.807501	-0.057249	4.815617
280.972590	8000.532850	10.812506	-0.057272	4.815621
280.977311	8000.457065	10.817511	-0.057273	4.815599
280.824402	8000.529337	10.822515	-0.057245	4.815621
280.848561	8000.558581	10.827520	-0.057249	4.815629
280.795974	8000.538480	10.832525	-0.057239	4.815624
280.710922	8000.497545	10.837530	-0.057223	4.815612
281.003808	8000.441461	10.842535	-0.057278	4.815594
280.832146	8000.617065	10.847539	-0.057246	4.815646
280.698271	8000.595626	10.852544	-0.057221	4.815641
280.669987	8000.563105	10.857549	-0.057216	4.815631
280.843569	8000.461251	10.862554	-0.057248	4.815601
280.961277	8000.581784	10.867559	-0.057270	4.815636
280.777530	8000.609742	10.872563	-0.057236	4.815645
280.807534	8000.503388	10.877568	-0.057241	4.815613
280.768450	8000.540138	10.882573	-0.057234	4.815624
280.777801	8000.586233	10.887578	-0.057236	4.815638
280.716483	8000.530730	10.892583	-0.057224	4.815622
280.688627	8000.630703	10.897587	-0.057219	4.815651
280.885706	8000.432007	10.902592	-0.057255	4.815592
280.885532	8000.512135	10.907597	-0.057255	4.815616
280.718350	8000.613021	10.912602	-0.057224	4.815646
280.989140	8000.552300	10.917607	-0.057275	4.815627
280.747342	8000.511990	10.922611	-0.057230	4.815616
280.882541	8000.530239	10.927616	-0.057255	4.815621
281.037879	8000.528520	10.932621	-0.057284	4.815620
280.720402	8000.620521	10.937626	-0.057225	4.815648
280.893938	8000.426779	10.942631	-0.057257	4.815591
280.769692	8000.580726	10.947635	-0.057234	4.815636
280.877778	8000.546175	10.952640	-0.057254	4.815626
280.898898	8000.478139	10.957645	-0.057258	4.815606
280.808903	8000.547173	10.962650	-0.057241	4.815626
280.907509	8000.474001	10.967655	-0.057259	4.815604
280.776399	8000.523126	10.972659	-0.057235	4.815619
280.935131	8000.539627	10.977664	-0.057264	4.815623
280.931784	8000.523542	10.982669	-0.057264	4.815619
280.813784	8000.614553	10.987674	-0.057242	4.815646
280.986104	8000.528705	10.992679	-0.057274	4.815620
280.804805	8000.493664	10.997683	-0.057240	4.815611
280.756167	8000.520641	11.002688	-0.057231	4.815619
280.850795	8000.536086	11.007693	-0.057248	4.815623
280.891132	8000.583759	11.012698	-0.057256	4.815636
280.834238	8000.536876	11.017703	-0.057245	4.815623
280.740766	8000.626154	11.022707	-0.057228	4.815650
280.809145	8000.521500	11.027712	-0.057241	4.815619
280.819854	8000.531290	11.032717	-0.057243	4.815621
280.717976	8000.604402	11.037722	-0.057224	4.815643
280.800318	8000.514936	11.042727	-0.057239	4.815617
281.025440	8000.515434	11.047731	-0.057281	4.815616
281.068700	8000.611236	11.052736	-0.057289	4.815644
281.052774	8000.528700	11.057741	-0.057286	4.815620
280.954553	8000.560203	11.062746	-0.057267	4.815629
281.224868	8000.470625	11.067751	-0.057318	4.815602
280.972232	8000.600021	11.072755	-0.057271	4.815641
280.967065	8000.542237	11.077760	-0.057270	4.815624
280.985090	8000.550010	11.082765	-0.057273	4.815626
280.918563	8000.613020	11.087770	-0.057261	4.815645
280.838810	8000.450368	11.092775	-0.057246	4.815598
280.852367	8000.611925	11.097779	-0.057248	4.815645
280.868315	8000.434822	11.102784	-0.057251	4.815593
280.846817	8000.559474	11.107789	-0.057247	4.815630
280.966055	8000.504806	11.112794	-0.057269	4.815613
281.041645	8000.338301	11.117799	-0.057283	4.815564
281.084165	8000.593290	11.122803	-0.057291	4.815638
281.030646	8000.562490	11.127808	-0.057281	4.815630
281.082907	8000.527020	11.132813	-0.057291	4.815619
280.815087	8000.585647	11.137818	-0.057241	4.815637
280.832929	8000.511147	11.142823	-0.057244	4.815616
281.114191	8000.535006	11.147827	-0.057297	4.815621
280.955986	8000.563384	11.152832	-0.057267	4.815630
281.003487	8000.555616	11.157837	-0.057276	4.815628
280.813591	8000.484107	11.162842	-0.057241	4.815608
281.026027	8000.598720	11.167847	-0.057280	4.815640
280.924935	8000.514782	11.172851	-0.057261	4.815616
280.778287	8000.624554	11.177856	-0.057234	4.815649
280.946809	8000.531164	11.182861	-0.057265	4.815621
280.890629	8000.586865	11.187866	-0.057255	4.815637
280.829143	8000.512127	11.192871	-0.057243	4.815616
280.889888	8000.649886	11.197875	-0.057255	4.815656
281.045282	8000.475078	11.202880	-0.057283	4.815604
281.176342	8000.508218	11.207885	-0.057308	4.815613
280.810569	8000.558822	11.212890	-0.057240	4.815630
280.971805	8000.548652	11.217895	-0.057270	4.815626
280.759384	8000.617808	11.222899	-0.057230	4.815647
280.869254	8000.395239	11.227904	-0.057250	4.815582
281.062361	8000.643092	11.232909	-0.057287	4.815653
281.101358	8000.504831	11.237914	-0.057294	4.815612
281.007403	8000.529993	11.242919	-0.057276	4.815620
281.054282	8000.632266	11.247923	-0.057285	4.815650
281.144296	8000.521557	11.252928	-0.057302	4.815617
281.184693	8000.544657	11.257933	-0.057309	4.815624
280.867526	8000.577898	11.262938	-0.057250	4.815635
281.072372	8000.548145	11.267943	-0.057288	4.815625
280.963365	8000.607250	11.272947	-0.057268	4.815643
281.061013	8000.433628	11.277952	-0.057286	4.815592
281.186045	8000.639760	11.282957	-0.057309	4.815651
281.149300	8000.532305	11.287962	-0.057302	4.815620
280.952201	8000.498073	11.292967	-0.057266	4.815611
280.918214	8000.582987	11.297971	-0.057259	4.815636
280.926801	8000.570305	11.302976	-0.057261	4.815632
280.984439	8000.517828	11.307981	-0.057272	4.815617
281.120376	8000.572418	11.312986	-0.057297	4.815632
281.248656	8000.569185	11.317991	-0.057321	4.815631
281.339920	8000.498029	11.322995	-0.057338	4.815609
280.985396	8000.515696	11.328000	-0.057272	4.815616
281.108108	8000.539083	11.333005	-0.057294	4.815622
281.035855	8000.531480	11.338010	-0.057281	4.815621
281.007714	8000.548110	11.343015	-0.057276	4.815626
281.023201	8000.442585	11.348019	-0.057278	4.815595
280.995692	8000.480594	11.353024	-0.057273	4.815606
280.971369	8000.551777	11.358029	-0.057269	4.815627
280.875658	8000.509598	11.363034	-0.057251	4.815615
281.089216	8000.535548	11.368039	-0.057291	4.815621
281.036926	8000.640463	11.373043	-0.057281	4.815652
281.050905	8000.479353	11.378048	-0.057283	4.815605
281.130680	8000.539428	11.383053	-0.057298	4.815622
280.965941	8000.585863	11.388058	-0.057268	4.815637
281.019365	8000.509811	11.393063	-0.057278	4.815614
280.961075	8000.554792	11.398067	-0.057267	4.815628
281.094681	8000.474718	11.403072	-0.057291	4.815604
281.110637	8000.639521	11.408077	-0.057295	4.815652
280.882905	8000.539608	11.413082	-0.057252	4.815624
281.177363	8000.535905	11.418087	-0.057307	4.815621
281.264390	8000.522376	11.423091	-0.057323	4.815617
281.070988	8000.464699	11.428096	-0.057287	4.815601
281.051762	8000.613964	11.433101	-0.057283	4.815645
280.998363	8000.541495	11.438106	-0.057273	4.815624
281.079874	8000.494754	11.443111	-0.057288	4.815610
281.102637	8000.585945	11.448115	-0.057293	4.815636
281.326827	8000.538347	11.453120	-0.057334	4.815621
281.293417	8000.533521	11.458125	-0.057328	4.815620
281.053699	8000.579789	11.463130	-0.057284	4.815635
281.184894	8000.492196	11.468135	-0.057308	4.815608
281.457893	8000.541563	11.473139	-0.057359	4.815621
281.389061	8000.537222	11.478144	-0.057346	4.815621
281.378935	8000.548806	11.483149	-0.057344	4.815624
281.355641	8000.505681	11.488154	-0.057340	4.815611
281.311542	8000.567992	11.493159	-0.057331	4.815630
281.124588	8000.434559	11.498163	-0.057296	4.815592
281.370537	8000.637340	11.503168	-0.057342	4.815650
281.460644	8000.544795	11.508173	-0.057359	4.815622
281.337019	8000.498950	11.513178	-0.057336	4.815610
281.289253	8000.531284	11.518183	-0.057327	4.815619
281.203816	8000.533080	11.523187	-0.057311	4.815620
281.111035	8000.477059	11.528192	-0.057294	4.815604
281.261089	8000.630180	11.533197	-0.057322	4.815648
281.415813	8000.497029	11.538202	-0.057350	4.815609
281.520400	8000.534008	11.543207	-0.057370	4.815619
281.332746	8000.533053	11.548211	-0.057335	4.815620
281.350097	8000.531199	11.553216	-0.057338	4.815619
281.407425	8000.552441	11.558221	-0.057349	4.815625
281.245085	8000.460015	11.563226	-0.057319	4.815599
281.360405	8000.536703	11.568231	-0.057340	4.815621
281.417220	8000.502376	11.573235	-0.057351	4.815610
281.349376	8000.545064	11.578240	-0.057338	4.815623
281.542130	8000.489469	11.583245	-0.057374	4.815606
281.571940	8000.573298	11.588250	-0.057379	4.815630
281.496577	8000.623341	11.593255	-0.057365	4.815645
281.434620	8000.518677	11.598259	-0.057354	4.815615
281.413806	8000.589919	11.603264	-0.057350	4.815636
281.513101	8000.417391	11.608269	-0.057368	4.815585
281.373646	8000.635197	11.613274	-0.057342	4.815649
281.280997	8000.489426	11.618279	-0.057325	4.815607
281.647567	8000.593758	11.623283	-0.057393	4.815636
281.538227	8000.478697	11.628288	-0.057373	4.815603
281.369203	8000.544293	11.633293	-0.057341	4.815623
281.273167	8000.595064	11.638298	-0.057323	4.815638
281.484042	8000.504508	11.643303	-0.057363	4.815611
281.372565	8000.520834	11.648307	-0.057342	4.815616
281.306116	8000.568887	11.653312	-0.057329	4.815630
281.680875	8000.519494	11.658317	-0.057399	4.815614
281.222975	8000.581403	11.663322	-0.057314	4.815634
281.317401	8000.504957	11.668327	-0.057331	4.815611
281.447968	8000.522063	11.673331	-0.057356	4.815616
281.234117	8000.565552	11.678336	-0.057316	4.815630
281.434154	8000.517556	11.683341	-0.057353	4.815615
281.292214	8000.614584	11.688346	-0.057327	4.815644
281.385053	8000.504989	11.693351	-0.057344	4.815611
281.420095	8000.538686	11.698355	-0.057350	4.815621
281.422787	8000.525906	11.703360	-0.057351	4.815617
281.589779	8000.615199	11.708365	-0.057382	4.815642
281.397967	8000.529766	11.713370	-0.057346	4.815618
281.462604	8000.498774	11.718375	-0.057358	4.815609
281.546492	8000.558918	11.723379	-0.057374	4.815626
281.393103	8000.461297	11.728384	-0.057345	4.815598
281.498783	8000.448075	11.733389	-0.057365	4.815594
281.356083	8000.522653	11.738394	-0.057338	4.815616
281.353813	8000.527955	11.743399	-0.057338	4.815618
281.407081	8000.526693	11.748403	-0.057348	4.815617
281.577365	8000.558342	11.753408	-0.057379	4.815626
281.632680	8000.481252	11.758413	-0.057390	4.815603
281.372042	8000.471616	11.763418	-0.057341	4.815601
281.300889	8000.538824	11.768423	-0.057328	4.815621
281.350735	8000.392194	11.773427	-0.057337	4.815578
281.158895	8000.614479	11.778432	-0.057301	4.815644
281.249230	8000.479200	11.783437	-0.057318	4.815604
281.299006	8000.554809	11.788442	-0.057327	4.815626
281.377658	8000.531527	11.793447	-0.057342	4.815619
281.177647	8000.543190	11.798451	-0.057305	4.815623
281.117501	8000.609510	11.803456	-0.057293	4.815643
281.507850	8000.521909	11.808461	-0.057366	4.815616
281.386276	8000.518837	11.813466	-0.057343	4.815615
281.323065	8000.525273	11.818471	-0.057332	4.815617
281.329627	8000.626883	11.823475	-0.057333	4.815647
281.389904	8000.606503	11.828480	-0.057344	4.815641
281.482181	8000.425312	11.833485	-0.057361	4.815587
281.385356	8000.641683	11.838490	-0.057343	4.815651
281.424013	8000.413665	11.843495	-0.057350	4.815584
281.421182	8000.534352	11.848499	-0.057350	4.815620
281.352252	8000.505434	11.853504	-0.057337	4.815611
281.359443	8000.524782	11.858509	-0.057338	4.815617
281.231510	8000.519468	11.863514	-0.057314	4.815616
281.352463	8000.431706	11.868519	-0.057337	4.815590
281.380911	8000.620222	11.873523	-0.057342	4.815645
281.386099	8000.500636	11.878528	-0.057343	4.815610
281.454220	8000.589369	11.883533	-0.057356	4.815636
281.405563	8000.516978	11.888538	-0.057347	4.815615
281.508903	8000.423583	11.893543	-0.057366	4.815587
281.626795	8000.648833	11.898547	-0.057388	4.815652
281.324691	8000.450463	11.903552	-0.057331	4.815596
281.514380	8000.544403	11.908557	-0.057367	4.815622
281.340053	8000.620596	11.913562	-0.057334	4.815645
281.540764	8000.514915	11.918567	-0.057372	4.815613
281.368555	8000.524898	11.923571	-0.057339	4.815617
281.362108	8000.533337	11.928576	-0.057338	4.815620
281.385747	8000.441836	11.933581	-0.057343	4.815593
281.315380	8000.531494	11.938586	-0.057329	4.815619
281.471639	8000.618474	11.943591	-0.057359	4.815644
281.502623	8000.516408	11.948595	-0.057364	4.815614
281.346896	8000.577949	11.953600	-0.057335	4.815633
281.568115	8000.570904	11.958605	-0.057376	4.815630
281.347892	8000.601467	11.963610	-0.057335	4.815640
281.389247	8000.515599	11.968615	-0.057343	4.815614
281.386217	8000.565765	11.973619	-0.057342	4.815629
281.474307	8000.510584	11.978624	-0.057359	4.815612
281.511987	8000.531502	11.983629	-0.057366	4.815618
281.413897	8000.622842	11.988634	-0.057348	4.815646
281.528513	8000.489030	11.993639	-0.057369	4.815606
281.674615	8000.528830	11.998643	-0.057396	4.815617
281.515901	8000.605281	12.003648	-0.057366	4.815640
281.307537	8000.436235	12.008653	-0.057328	4.815592
281.357099	8000.535347	12.013658	-0.057337	4.815620
281.254907	8000.361641	12.018663	-0.057318	4.815570
281.352604	8000.428422	12.023667	-0.057336	4.815589
281.489189	8000.574911	12.028672	-0.057361	4.815631
281.520484	8000.399126	12.033677	-0.057367	4.815580
281.294557	8000.577043	12.038682	-0.057325	4.815633
281.417182	8000.467939	12.043687	-0.057348	4.815600
281.486284	8000.598359	12.048691	-0.057361	4.815638
281.407497	8000.541498	12.053696	-0.057346	4.815622
281.704458	8000.488688	12.058701	-0.057401	4.815605
281.519596	8000.558297	12.063706	-0.057367	4.815626
281.600845	8000.519031	12.068711	-0.057382	4.815614
281.581982	8000.512307	12.073715	-0.057378	4.815612
281.623386	8000.554656	12.078720	-0.057386	4.815625
281.716330	8000.422625	12.083725	-0.057403	4.815586
281.381476	8000.523956	12.088730	-0.057341	4.815617
281.433377	8000.478864	12.093735	-0.057350	4.815603
281.625327	8000.540788	12.098739	-0.057386	4.815621
281.500516	8000.579332	12.103744	-0.057363	4.815632
281.464676	8000.430222	12.108749	-0.057356	4.815589
281.464970	8000.571262	12.113754	-0.057356	4.815630
281.460960	8000.519907	12.118759	-0.057355	4.815615
281.518718	8000.425762	12.123763	-0.057366	4.815587
281.642863	8000.600895	12.128768	-0.057389	4.815638
281.750675	8000.494752	12.133773	-0.057409	4.815606
281.579601	8000.562452	12.138778	-0.057377	4.815627
281.673641	8000.483862	12.143783	-0.057395	4.815604
281.720060	8000.545527	12.148787	-0.057404	4.815621
281.677964	8000.529872	12.153792	-0.057396	4.815617
281.659070	8000.546654	12.158797	-0.057392	4.815622
281.686911	8000.564206	12.163802	-0.057397	4.815627
281.682077	8000.441249	12.168807	-0.057396	4.815591
281.720536	8000.539111	12.173811	-0.057403	4.815620
281.756589	8000.590989	12.178816	-0.057410	4.815635
281.766680	8000.522770	12.183821	-0.057412	4.815615
281.698342	8000.646654	12.188826	-0.057399	4.815651
281.523588	8000.485639	12.193831	-0.057367	4.815605
281.659008	8000.508167	12.198835	-0.057392	4.815611
281.557112	8000.504350	12.203840	-0.057373	4.815610
281.566238	8000.614550	12.208845	-0.057375	4.815642
281.623378	8000.524668	12.213850	-0.057385	4.815616
281.669932	8000.495515	12.218855	-0.057394	4.815607
281.808642	8000.543741	12.223859	-0.057420	4.815621
281.753200	8000.575948	12.228864	-0.057409	4.815630
281.685497	8000.518201	12.233869	-0.057397	4.815614
281.481991	8000.607805	12.238874	-0.057359	4.815641
281.608587	8000.569285	12.243879	-0.057382	4.815629
281.809889	8000.556570	12.248883	-0.057420	4.815624
281.765116	8000.467147	12.253888	-0.057411	4.815598
281.703593	8000.515281	12.258893	-0.057400	4.815613
281.480240	8000.511601	12.263898	-0.057358	4.815613
281.598150	8000.574442	12.268903	-0.057380	4.815631
281.568965	8000.552590	12.273907	-0.057375	4.815624
281.527635	8000.474977	12.278912	-0.057367	4.815602
281.760127	8000.570691	12.283917	-0.057410	4.815629
281.459789	8000.608482	12.288922	-0.057354	4.815641
281.638067	8000.407337	12.293927	-0.057387	4.815582
281.903683	8000.545267	12.298931	-0.057437	4.815621
281.615253	8000.511666	12.303936	-0.057383	4.815612
281.639263	8000.493894	12.308941	-0.057388	4.815607
281.559705	8000.537458	12.313946	-0.057373	4.815620
281.660205	8000.529494	12.318951	-0.057391	4.815617
281.819966	8000.536396	12.323955	-0.057421	4.815618
281.753963	8000.554539	12.328960	-0.057409	4.815624
281.929139	8000.446299	12.333965	-0.057441	4.815592
281.810159	8000.607814	12.338970	-0.057419	4.815639
281.688805	8000.564143	12.343975	-0.057397	4.815627
281.764961	8000.430766	12.348979	-0.057411	4.815588
281.719354	8000.512285	12.353984	-0.057402	4.815612
281.735654	8000.526441	12.358989	-0.057405	4.815616
281.842685	8000.591241	12.363994	-0.057425	4.815634
281.778870	8000.470518	12.368999	-0.057413	4.815599
281.715832	8000.584873	12.374003	-0.057401	4.815633
281.656696	8000.579623	12.379008	-0.057390	4.815632
281.658434	8000.510198	12.384013	-0.057391	4.815611
281.579179	8000.616806	12.389018	-0.057376	4.815643
281.694095	8000.442398	12.394023	-0.057397	4.815592
281.681586	8000.573611	12.399027	-0.057395	4.815630
281.806093	8000.525440	12.404032	-0.057418	4.815615
281.719148	8000.531486	12.409037	-0.057402	4.815617
281.648822	8000.549557	12.414042	-0.057389	4.815623
281.666345	8000.446202	12.419047	-0.057392	4.815593
281.648137	8000.521761	12.424051	-0.057389	4.815615
281.583915	8000.554892	12.429056	-0.057377	4.815625
281.682656	8000.518050	12.434061	-0.057395	4.815614
281.473750	8000.593674	12.439066	-0.057356	4.815637
281.382841	8000.422289	12.444071	-0.057339	4.815587
281.551224	8000.503056	12.449075	-0.057370	4.815610
281.617807	8000.597107	12.454080	-0.057383	4.815637
281.678743	8000.583149	12.459085	-0.057394	4.815633
281.684055	8000.510578	12.464090	-0.057395	4.815611
281.493276	8000.564063	12.469095	-0.057359	4.815628
281.535219	8000.512396	12.474099	-0.057367	4.815613
281.535273	8000.557270	12.479104	-0.057367	4.815626
281.576224	8000.571832	12.484109	-0.057375	4.815630
281.579575	8000.520598	12.489114	-0.057375	4.815615
281.510208	8000.586767	12.494119	-0.057362	4.815635
281.742186	8000.522202	12.499123	-0.057406	4.815615
281.663249	8000.582871	12.504128	-0.057391	4.815633
281.676619	8000.551034	12.509133	-0.057393	4.815623
281.585182	8000.477938	12.514138	-0.057376	4.815602
281.723855	8000.559286	12.519143	-0.057402	4.815626
281.878429	8000.610979	12.524147	-0.057431	4.815640
281.720681	8000.598762	12.529152	-0.057401	4.815637
281.658285	8000.417160	12.534157	-0.057390	4.815584
281.843589	8000.633904	12.539162	-0.057424	4.815647
281.688060	8000.504191	12.544167	-0.057395	4.815610
281.834558	8000.572846	12.549171	-0.057423	4.815629
281.773476	8000.532304	12.554176	-0.057411	4.815617
281.597985	8000.492016	12.559181	-0.057378	4.815606
281.601987	8000.583967	12.564186	-0.057379	4.815633
281.710545	8000.609259	12.569191	-0.057399	4.815640
281.900821	8000.505542	12.574195	-0.057435	4.815609
281.573456	8000.495875	12.579200	-0.057374	4.815608
281.645237	8000.504534	12.584205	-0.057387	4.815610
281.694886	8000.556635	12.589210	-0.057396	4.815625
281.610474	8000.475107	12.594215	-0.057380	4.815601
281.522589	8000.532424	12.599219	-0.057364	4.815619
281.554693	8000.574620	12.604224	-0.057370	4.815631
281.548299	8000.500788	12.609229	-0.057369	4.815609
281.475574	8000.560490	12.614234	-0.057355	4.815627
281.725774	8000.521868	12.619239	-0.057402	4.815615
281.780423	8000.582600	12.624243	-0.057412	4.815632
281.456575	8000.533458	12.629248	-0.057352	4.815619
281.650052	8000.466122	12.634253	-0.057388	4.815599
281.759605	8000.566223	12.639258	-0.057408	4.815627
281.695941	8000.604705	12.644263	-0.057396	4.815639
281.737386	8000.485716	12.649267	-0.057404	4.815604
281.654542	8000.532431	12.654272	-0.057388	4.815618
281.868995	8000.594726	12.659277	-0.057428	4.815635
281.750403	8000.488059	12.664282	-0.057406	4.815605
281.861951	8000.572166	12.669287	-0.057427	4.815629
281.865949	8000.478203	12.674291	-0.057428	4.815601
281.607089	8000.522020	12.679296	-0.057379	4.815615
281.640821	8000.585613	12.684301	-0.057386	4.815634
281.730487	8000.604182	12.689306	-0.057402	4.815639
281.723707	8000.468372	12.694311	-0.057401	4.815599
281.789920	8000.615840	12.699315	-0.057413	4.815642
281.573977	8000.546036	12.704320	-0.057373	4.815622
281.822321	8000.476398	12.709325	-0.057419	4.815601
281.688569	8000.621643	12.714330	-0.057394	4.815644
281.746863	8000.584135	12.719335	-0.057405	4.815633
281.951929	8000.513784	12.724339	-0.057443	4.815611
281.714419	8000.528035	12.729344	-0.057399	4.815616
281.825675	8000.515974	12.734349	-0.057420	4.815612
281.749796	8000.526475	12.739354	-0.057406	4.815616
281.963706	8000.526790	12.744359	-0.057445	4.815615
281.847700	8000.519534	12.749363	-0.057424	4.815613
281.712680	8000.615608	12.754368	-0.057399	4.815642
281.792900	8000.526106	12.759373	-0.057414	4.815616
281.742293	8000.539160	12.764378	-0.057404	4.815620
281.544217	8000.634196	12.769383	-0.057367	4.815648
281.666558	8000.546456	12.774387	-0.057390	4.815622
281.735352	8000.547586	12.779392	-0.057403	4.815622
281.843517	8000.520516	12.784397	-0.057423	4.815614
281.898513	8000.511802	12.789402	-0.057433	4.815611
281.822559	8000.618465	12.794407	-0.057419	4.815642
281.859382	8000.547481	12.799411	-0.057426	4.815621
281.949172	8000.530793	12.804416	-0.057442	4.815616
281.932725	8000.536930	12.809421	-0.057439	4.815618
281.667623	8000.537905	12.814426	-0.057390	4.815620
281.603012	8000.502647	12.819431	-0.057378	4.815610
281.893491	8000.520249	12.824435	-0.057432	4.815613
281.896409	8000.645307	12.829440	-0.057432	4.815650
281.811285	8000.407769	12.834445	-0.057416	4.815581
281.751016	8000.599099	12.839450	-0.057405	4.815637
281.997320	8000.535839	12.844455	-0.057451	4.815617
281.923237	8000.527137	12.849459	-0.057437	4.815615
281.818844	8000.592729	12.854464	-0.057418	4.815635
281.873073	8000.526305	12.859469	-0.057428	4.815615
281.950045	8000.474146	12.864474	-0.057442	4.815600
281.620524	8000.511457	12.869479	-0.057381	4.815612
282.044480	8000.432957	12.874483	-0.057460	4.815587
281.981609	8000.521671	12.879488	-0.057448	4.815613
281.954180	8000.604559	12.884493	-0.057443	4.815638
282.006728	8000.524217	12.889498	-0.057453	4.815614
281.921242	8000.562340	12.894503	-0.057437	4.815626
281.940600	8000.563725	12.899507	-0.057440	4.815626
281.861550	8000.476942	12.904512	-0.057425	4.815601
282.017539	8000.498741	12.909517	-0.057454	4.815606
281.772679	8000.629334	12.914522	-0.057409	4.815646
281.762340	8000.462479	12.919527	-0.057407	4.815597
281.877107	8000.622501	12.924531	-0.057428	4.815643
281.863119	8000.532516	12.929536	-0.057426	4.815617
281.848080	8000.473499	12.934541	-0.057423	4.815600
281.928274	8000.518625	12.939546	-0.057438	4.815613
282.242503	8000.517386	12.944551	-0.057496	4.815611
282.035467	8000.522522	12.949555	-0.057458	4.815613
281.698017	8000.602440	12.954560	-0.057395	4.815638
281.903371	8000.434863	12.959565	-0.057433	4.815588
281.989811	8000.514283	12.964570	-0.057449	4.815611
281.905609	8000.492592	12.969575	-0.057433	4.815605
281.982173	8000.624205	12.974579	-0.057448	4.815643
281.897214	8000.549078	12.979584	-0.057432	4.815622
281.918061	8000.469283	12.984589	-0.057435	4.815598
281.967769	8000.534208	12.989594	-0.057445	4.815617
282.016201	8000.544619	12.994599	-0.057454	4.815620
282.079270	8000.534970	12.999603	-0.057465	4.815617
281.824018	8000.603421	13.004608	-0.057418	4.815638
281.971896	8000.524649	13.009613	-0.057445	4.815614
282.018484	8000.545715	13.014618	-0.057454	4.815620
281.892433	8000.436789	13.019623	-0.057430	4.815589
281.854480	8000.629555	13.024627	-0.057423	4.815646
282.003994	8000.525167	13.029632	-0.057451	4.815614
282.002854	8000.469585	13.034637	-0.057451	4.815598
281.874922	8000.628816	13.039642	-0.057427	4.815645
281.993644	8000.497208	13.044647	-0.057449	4.815606
282.141344	8000.626788	13.049651	-0.057477	4.815643
282.103341	8000.511831	13.054656	-0.057470	4.815610
282.224937	8000.502078	13.059661	-0.057492	4.815606
282.034447	8000.533129	13.064666	-0.057457	4.815616
282.026788	8000.573603	13.069671	-0.057455	4.815628
282.138777	8000.524158	13.074675	-0.057476	4.815613
282.060611	8000.566675	13.079680	-0.057461	4.815626
282.099660	8000.391017	13.084685	-0.057469	4.815575
282.130590	8000.634069	13.089690	-0.057474	4.815646
282.144629	8000.478299	13.094695	-0.057477	4.815600
281.986552	8000.597500	13.099699	-0.057448	4.815636
281.920567	8000.520548	13.104704	-0.057435	4.815613
281.971065	8000.502145	13.109709	-0.057445	4.815608
282.069054	8000.403319	13.114714	-0.057463	4.815578
281.875776	8000.527282	13.119719	-0.057427	4.815616
282.144085	8000.516739	13.124723	-0.057477	4.815611
282.158244	8000.543682	13.129728	-0.057479	4.815619
282.106084	8000.386823	13.134733	-0.057470	4.815573
281.952453	8000.568068	13.139738	-0.057441	4.815627
282.005825	8000.462097	13.144743	-0.057451	4.815596
282.159366	8000.509499	13.149747	-0.057479	4.815609
282.046572	8000.580295	13.154752	-0.057458	4.815630
282.150549	8000.492252	13.159757	-0.057478	4.815604
282.192290	8000.520718	13.164762	-0.057485	4.815612
282.131503	8000.507961	13.169767	-0.057474	4.815609
282.208984	8000.534878	13.174771	-0.057489	4.815616
282.165297	8000.569416	13.179776	-0.057480	4.815626
282.038644	8000.505355	13.184781	-0.057457	4.815608
282.079902	8000.574415	13.189786	-0.057464	4.815628
282.056185	8000.509913	13.194791	-0.057460	4.815610
282.223965	8000.433606	13.199795	-0.057491	4.815587
282.024093	8000.615159	13.204800	-0.057454	4.815641
282.134417	8000.487687	13.209805	-0.057474	4.815603
282.307741	8000.541826	13.214810	-0.057507	4.815618
282.238534	8000.532135	13.219815	-0.057494	4.815615
282.079921	8000.497466	13.224819	-0.057464	4.815606
282.143746	8000.518816	13.229824	-0.057476	4.815612
282.245313	8000.610239	13.234829	-0.057495	4.815638
282.104338	8000.551285	13.239834	-0.057469	4.815621
281.940748	8000.434261	13.244839	-0.057438	4.815588
281.976052	8000.527797	13.249843	-0.057445	4.815615
281.972573	8000.646339	13.254848	-0.057444	4.815650
281.972586	8000.508502	13.259853	-0.057444	4.815610
282.058723	8000.539835	13.264858	-0.057460	4.815618
281.959880	8000.554232	13.269863	-0.057442	4.815623
282.022043	8000.406735	13.274867	-0.057453	4.815580
282.045585	8000.544954	13.279872	-0.057457	4.815620
282.035328	8000.384511	13.284877	-0.057455	4.815573
282.040479	8000.507468	13.289882	-0.057456	4.815609
282.264898	8000.462010	13.294887	-0.057498	4.815595
282.201409	8000.330608	13.299891	-0.057486	4.815557
282.237735	8000.558790	13.304896	-0.057493	4.815623
282.069258	8000.535712	13.309901	-0.057462	4.815617
282.237978	8000.445529	13.314906	-0.057493	4.815590
282.141748	8000.551859	13.319911	-0.057475	4.815621
282.311138	8000.427496	13.324915	-0.057507	4.815584
282.140894	8000.459950	13.329920	-0.057475	4.815595
282.105159	8000.400593	13.334925	-0.057468	4.815577
282.067060	8000.515358	13.339930	-0.057461	4.815611
282.171074	8000.461508	13.344935	-0.057480	4.815595
282.361789	8000.539440	13.349939	-0.057516	4.815617
282.263432	8000.504694	13.354944	-0.057498	4.815607
282.070775	8000.615847	13.359949	-0.057462	4.815641
282.233567	8000.445431	13.364954	-0.057492	4.815590
282.179293	8000.488342	13.369959	-0.057482	4.815603
282.145736	8000.390555	13.374963	-0.057475	4.815574
282.048361	8000.629357	13.379968	-0.057457	4.815645
282.300275	8000.482847	13.384973	-0.057504	4.815601
282.220324	8000.526404	13.389978	-0.057489	4.815614
282.135904	8000.476930	13.394983	-0.057474	4.815600
282.296788	8000.514836	13.399987	-0.057504	4.815610
282.153531	8000.621460	13.404992	-0.057477	4.815642
282.202618	8000.489774	13.409997	-0.057486	4.815603
282.285970	8000.538157	13.415002	-0.057501	4.815617
282.327932	8000.540983	13.420007	-0.057509	4.815617
282.364145	8000.449687	13.425011	-0.057516	4.815591
282.190690	8000.471403	13.430016	-0.057484	4.815598
282.282837	8000.462233	13.435021	-0.057501	4.815595
282.116209	8000.569540	13.440026	-0.057470	4.815627
282.137478	8000.608353	13.445031	-0.057474	4.815638
282.229524	8000.433566	13.450035	-0.057491	4.815587
282.070983	8000.565582	13.455040	-0.057461	4.815626
282.140256	8000.392558	13.460045	-0.057474	4.815575
282.228923	8000.516890	13.465050	-0.057491	4.815611
282.443944	8000.573854	13.470055	-0.057531	4.815626
282.367268	8000.430479	13.475059	-0.057516	4.815585
282.215463	8000.636331	13.480064	-0.057488	4.815646
282.131036	8000.491761	13.485069	-0.057472	4.815604
282.019076	8000.541202	13.490074	-0.057451	4.815619
282.211074	8000.559320	13.495079	-0.057487	4.815623
282.318052	8000.534367	13.500083	-0.057507	4.815616
282.226496	8000.600171	13.505088	-0.057490	4.815635
282.102804	8000.498762	13.510093	-0.057467	4.815606
281.952402	8000.528337	13.515098	-0.057439	4.815616
282.276863	8000.590308	13.520103	-0.057499	4.815632
282.286501	8000.412027	13.525107	-0.057501	4.815580
282.085128	8000.535858	13.530112	-0.057463	4.815617
282.179681	8000.602590	13.535117	-0.057481	4.815636
282.328518	8000.399890	13.540122	-0.057509	4.815576
282.120319	8000.535361	13.545127	-0.057470	4.815617
282.032520	8000.568104	13.550131	-0.057453	4.815627
281.991310	8000.546053	13.555136	-0.057446	4.815621
282.188985	8000.409335	13.560141	-0.057482	4.815580
282.186270	8000.519341	13.565146	-0.057482	4.815612
281.879975	8000.597636	13.570151	-0.057425	4.815636
282.151960	8000.502743	13.575155	-0.057476	4.815607
282.123246	8000.428543	13.580160	-0.057470	4.815586
282.097024	8000.458026	13.585165	-0.057465	4.815594
282.129458	8000.615624	13.590170	-0.057471	4.815640
282.091100	8000.504936	13.595175	-0.057464	4.815608
281.993676	8000.555685	13.600179	-0.057446	4.815623
281.958053	8000.501672	13.605184	-0.057439	4.815608
282.031612	8000.481511	13.610189	-0.057453	4.815601
282.019383	8000.525114	13.615194	-0.057451	4.815614
282.046140	8000.620647	13.620199	-0.057456	4.815642
282.251734	8000.444525	13.625203	-0.057494	4.815590
282.044309	8000.613133	13.630208	-0.057455	4.815640
282.006591	8000.454374	13.635213	-0.057448	4.815594
282.139591	8000.622176	13.640218	-0.057473	4.815642
282.078621	8000.534622	13.645223	-0.057461	4.815617
282.151086	8000.467430	13.650227	-0.057475	4.815597
282.203351	8000.423412	13.655232	-0.057485	4.815584
282.329513	8000.538746	13.660237	-0.057508	4.815617
282.372937	8000.505267	13.665242	-0.057516	4.815607
282.156411	8000.527342	13.670247	-0.057476	4.815614
282.348817	8000.518755	13.675251	-0.057512	4.815611
282.307144	8000.539436	13.680256	-0.057504	4.815617
282.288486	8000.518825	13.685261	-0.057500	4.815611
282.244630	8000.571524	13.690266	-0.057492	4.815627
282.126057	8000.474474	13.695271	-0.057470	4.815599
282.185327	8000.517118	13.700275	-0.057481	4.815611
282.105915	8000.526492	13.705280	-0.057466	4.815614
282.179964	8000.448641	13.710285	-0.057480	4.815591
282.076477	8000.435181	13.715290	-0.057461	4.815588
282.106616	8000.514743	13.720295	-0.057466	4.815611
282.270247	8000.516366	13.725299	-0.057497	4.815611
282.159201	8000.566891	13.730304	-0.057476	4.815626
282.221356	8000.384133	13.735309	-0.057487	4.815572
282.351346	8000.513420	13.740314	-0.057512	4.815609
282.232751	8000.609765	13.745319	-0.057490	4.815638
282.199094	8000.525866	13.750323	-0.057483	4.815614
282.362751	8000.549929	13.755328	-0.057514	4.815620
282.334014	8000.459700	13.760333	-0.057508	4.815594
282.263547	8000.533331	13.765338	-0.057495	4.815616
281.986760	8000.504195	13.770343	-0.057444	4.815608
282.211097	8000.601913	13.775347	-0.057485	4.815636
282.334601	8000.563342	13.780352	-0.057508	4.815624
282.194012	8000.431738	13.785357	-0.057482	4.815586
282.413768	8000.528312	13.790362	-0.057523	4.815613
282.039896	8000.564892	13.795367	-0.057453	4.815626
282.174987	8000.479498	13.800371	-0.057478	4.815600
282.366506	8000.529663	13.805376	-0.057514	4.815614
282.177475	8000.488082	13.810381	-0.057479	4.815603
282.111525	8000.566061	13.815386	-0.057467	4.815626
282.115669	8000.467826	13.820391	-0.057467	4.815597
282.393031	8000.535432	13.825395	-0.057519	4.815616
282.063885	8000.622967	13.830400	-0.057458	4.815643
281.966490	8000.440787	13.835405	-0.057439	4.815590
282.294484	8000.563719	13.840410	-0.057501	4.815624
282.361920	8000.533841	13.845415	-0.057513	4.815615
282.492419	8000.502864	13.850419	-0.057537	4.815606
282.307460	8000.622692	13.855424	-0.057503	4.815641
282.339545	8000.513163	13.860429	-0.057509	4.815609
282.265590	8000.535449	13.865434	-0.057495	4.815616
282.242886	8000.600250	13.870439	-0.057491	4.815635
282.362989	8000.500719	13.875443	-0.057513	4.815606
282.335929	8000.522709	13.880448	-0.057508	4.815612
282.510361	8000.514895	13.885453	-0.057540	4.815609
282.534441	8000.499261	13.890458	-0.057545	4.815604
282.285300	8000.565676	13.895463	-0.057498	4.815625
282.298276	8000.436600	13.900467	-0.057501	4.815587
282.179921	8000.606674	13.905472	-0.057479	4.815637
282.338537	8000.499230	13.910477	-0.057508	4.815605
282.219403	8000.562443	13.915482	-0.057486	4.815624
282.199730	8000.517240	13.920487	-0.057482	4.815611
282.408135	8000.421300	13.925491	-0.057521	4.815582
282.330969	8000.574957	13.930496	-0.057507	4.815627
282.431035	8000.474028	13.935501	-0.057525	4.815597
282.489908	8000.547652	13.940506	-0.057536	4.815619
282.418673	8000.541134	13.945511	-0.057523	4.815617
282.213239	8000.403119	13.950515	-0.057485	4.815578
282.138719	8000.631613	13.955520	-0.057471	4.815645
282.256044	8000.502119	13.960525	-0.057493	4.815606
282.214315	8000.553785	13.965530	-0.057485	4.815622
282.217284	8000.514297	13.970535	-0.057485	4.815610
282.180779	8000.525447	13.975539	-0.057479	4.815614
282.192348	8000.536320	13.980544	-0.057481	4.815617
282.097656	8000.495224	13.985549	-0.057463	4.815605
282.323081	8000.446578	13.990554	-0.057505	4.815590
282.366229	8000.581915	13.995559	-0.057513	4.815629
282.267884	8000.536485	14.000563	-0.057495	4.815616
282.116696	8000.558567	14.005568	-0.057466	4.815624
282.267846	8000.503356	14.010573	-0.057495	4.815607
282.308819	8000.504028	14.015578	-0.057502	4.815607
282.307800	8000.601241	14.020583	-0.057502	4.815635
282.406455	8000.484261	14.025587	-0.057520	4.815601
282.176643	8000.544583	14.030592	-0.057477	4.815619
282.147626	8000.564403	14.035597	-0.057472	4.815625
282.349680	8000.516441	14.040602	-0.057510	4.815610
282.096516	8000.616981	14.045607	-0.057462	4.815641
282.180717	8000.437791	14.050611	-0.057478	4.815588
282.183953	8000.524389	14.055616	-0.057479	4.815613
282.348523	8000.534576	14.060621	-0.057509	4.815616
282.432436	8000.452613	14.065626	-0.057525	4.815591
282.201106	8000.610142	14.070631	-0.057482	4.815638
282.301699	8000.508153	14.075635	-0.057500	4.815608
282.392095	8000.535283	14.080640	-0.057517	4.815616
282.318139	8000.542610	14.085645	-0.057503	4.815618
282.526544	8000.566342	14.090650	-0.057542	4.815624
282.288192	8000.514331	14.095655	-0.057498	4.815610
282.321044	8000.425117	14.100659	-0.057504	4.815584
282.098938	8000.551812	14.105664	-0.057463	4.815622
282.268747	8000.457374	14.110669	-0.057494	4.815593
282.497829	8000.524184	14.115674	-0.057537	4.815612
282.352274	8000.606195	14.120679	-0.057510	4.815636
282.539373	8000.429768	14.125683	-0.057544	4.815584
282.401433	8000.439247	14.130688	-0.057519	4.815587
282.153516	8000.492860	14.135693	-0.057472	4.815604
282.372571	8000.355425	14.140698	-0.057513	4.815563
282.492072	8000.562540	14.145703	-0.057536	4.815623
282.232609	8000.516593	14.150707	-0.057487	4.815611
282.215620	8000.498146	14.155712	-0.057484	4.815606
282.503211	8000.532797	14.160717	-0.057537	4.815614
282.562103	8000.436532	14.165722	-0.057548	4.815586
282.271799	8000.661474	14.170727	-0.057494	4.815653
282.422148	8000.483372	14.175731	-0.057522	4.815600
282.434245	8000.538062	14.180736	-0.057525	4.815616
282.225593	8000.608349	14.185741	-0.057486	4.815638
282.241978	8000.388508	14.190746	-0.057489	4.815573
282.290456	8000.573083	14.195751	-0.057498	4.815627
282.372165	8000.507111	14.200755	-0.057513	4.815607
282.264113	8000.533110	14.205760	-0.057493	4.815616
282.384530	8000.620570	14.210765	-0.057515	4.815641
282.546046	8000.455474	14.215770	-0.057545	4.815592
282.325583	8000.546936	14.220775	-0.057504	4.815619
282.463009	8000.497910	14.225779	-0.057530	4.815604
282.345529	8000.530164	14.230784	-0.057508	4.815614
282.313028	8000.549927	14.235789	-0.057502	4.815620
282.391036	8000.463593	14.240794	-0.057516	4.815595
282.457327	8000.521312	14.245799	-0.057528	4.815611
282.435553	7999.445017	14.250803	-0.057524	4.815297
282.340004	7996.242776	14.255808	-0.057504	4.814361
282.443478	7990.661871	14.260813	-0.057519	4.812730
282.511847	7983.965717	14.265818	-0.057528	4.810771
282.248271	7976.658830	14.270823	-0.057474	4.808635
282.155137	7969.031636	14.275827	-0.057451	4.806403
282.265864	7961.228917	14.280832	-0.057467	4.804118
282.047617	7953.299116	14.285837	-0.057421	4.801795
282.155652	7945.397349	14.290842	-0.057436	4.799479
282.017933	7937.402027	14.295847	-0.057405	4.797135
282.168751	7929.394716	14.300851	-0.057428	4.794785
282.180001	7921.375428	14.305856	-0.057425	4.792431
281.979443	7913.399555	14.310861	-0.057382	4.790089
281.816193	7905.408012	14.315866	-0.057347	4.787742
281.740412	7897.373902	14.320871	-0.057327	4.785381
281.897707	7889.379906	14.325875	-0.057351	4.783029
281.772357	7881.406104	14.330880	-0.057323	4.780683
281.702982	7873.390373	14.335885	-0.057305	4.778323
281.737821	7865.405445	14.340890	-0.057306	4.775971
281.685457	7857.387301	14.345895	-0.057291	4.773608
281.755802	7849.370493	14.350899	-0.057299	4.771244
281.616650	7841.380392	14.355904	-0.057268	4.768888
281.534822	7833.307237	14.360909	-0.057247	4.766505
281.854788	7825.401625	14.365914	-0.057301	4.764170
281.634247	7817.401355	14.370919	-0.057255	4.761807
281.626258	7809.354867	14.375923	-0.057248	4.759429
281.566479	7801.434241	14.380928	-0.057232	4.757087
281.446877	7793.330142	14.385933	-0.057204	4.754689
281.484031	7785.342660	14.390938	-0.057206	4.752325
281.371373	7777.267912	14.395943	-0.057180	4.749934
281.506655	7769.335857	14.400947	-0.057200	4.747583
281.278076	7761.281677	14.405952	-0.057152	4.745196
281.319334	7753.341807	14.410957	-0.057154	4.742840
281.451084	7745.318458	14.415962	-0.057174	4.740459
281.216564	7737.337450	14.420967	-0.057125	4.738090
281.162236	7729.326593	14.425971	-0.057109	4.735710
281.263318	7721.300297	14.430976	-0.057123	4.733325
281.103464	7713.281834	14.435981	-0.057088	4.730941
281.209016	7705.310870	14.440986	-0.057102	4.728569
281.136046	7697.259409	14.445991	-0.057084	4.726172
281.063948	7689.310590	14.450995	-0.057065	4.723805
280.894043	7681.341891	14.456000	-0.057028	4.721431
280.785982	7673.271013	14.461005	-0.057003	4.719025
280.993710	7665.374367	14.466010	-0.057036	4.716670
280.901221	7657.278331	14.471015	-0.057014	4.714254
280.945548	7649.284799	14.476019	-0.057017	4.711867
280.781648	7641.276973	14.481024	-0.056981	4.709475
280.919804	7633.242158	14.486029	-0.057001	4.707073
280.886611	7625.263366	14.491034	-0.056990	4.704688
280.698165	7617.344905	14.496039	-0.056950	4.702319
280.776295	7609.296828	14.501043	-0.056959	4.699910
280.589698	7601.336513	14.506048	-0.056919	4.697526
280.732111	7593.298120	14.511053	-0.056940	4.695117
280.846264	7585.294859	14.516058	-0.056956	4.692718
280.692435	7577.231555	14.521063	-0.056922	4.690299
280.635846	7569.297867	14.526067	-0.056907	4.687918
280.712451	7561.251553	14.531072	-0.056916	4.685502
280.503331	7553.311653	14.536077	-0.056871	4.683117
280.505423	7545.318886	14.541082	-0.056867	4.680715
280.432146	7537.302848	14.546087	-0.056848	4.678305
280.458028	7529.264509	14.551091	-0.056847	4.675886
280.317496	7521.234702	14.556096	-0.056816	4.673469
280.148936	7513.150950	14.561101	-0.056779	4.671034
280.242445	7505.200055	14.566106	-0.056791	4.668638
280.140946	7497.163351	14.571111	-0.056767	4.666215
280.067218	7489.201341	14.576115	-0.056748	4.663813
280.056354	7481.249918	14.581120	-0.056741	4.661414
279.964160	7473.196875	14.586125	-0.056719	4.658982
280.130249	7465.272954	14.591130	-0.056744	4.656588
279.859185	7457.216343	14.596135	-0.056689	4.654152
280.090249	7449.231676	14.601139	-0.056726	4.651737
280.101426	7441.225677	14.606144	-0.056723	4.649315
279.814579	7433.202422	14.611149	-0.056664	4.646886
279.852670	7425.209036	14.616154	-0.056666	4.644464
279.747526	7417.225654	14.621159	-0.056642	4.642045
279.769126	7409.228231	14.626163	-0.056640	4.639619
279.770850	7401.288444	14.631168	-0.056635	4.637211
279.833671	7393.213064	14.636173	-0.056642	4.634759
279.793147	7385.188023	14.641178	-0.056629	4.632322
279.671893	7377.151711	14.646183	-0.056601	4.629880
279.836006	7369.155963	14.651187	-0.056626	4.627449
279.880695	7361.178608	14.656192	-0.056630	4.625022
279.706762	7353.238073	14.661197	-0.056592	4.622605
279.514107	7345.197209	14.666202	-0.056551	4.620157
279.444904	7337.199670	14.671207	-0.056533	4.617720
279.529227	7329.156252	14.676211	-0.056543	4.615268
279.458234	7321.183595	14.681216	-0.056525	4.612836
279.417955	7313.133353	14.686221	-0.056512	4.610379
279.499174	7305.183470	14.691226	-0.056522	4.607952
279.293245	7297.110204	14.696231	-0.056478	4.605486
279.227813	7289.195435	14.701235	-0.056461	4.603066
279.264440	7281.171479	14.706240	-0.056462	4.600613
279.053495	7273.176562	14.711245	-0.056418	4.598166
279.083999	7265.210135	14.716250	-0.056418	4.595727
279.041947	7257.112525	14.721255	-0.056405	4.593247
279.117508	7249.064940	14.726259	-0.056414	4.590780
279.123275	7241.122559	14.731264	-0.056410	4.588345
279.150158	7233.120266	14.736269	-0.056410	4.585890
279.140943	7225.161994	14.741274	-0.056403	4.583447
278.841428	7217.120290	14.746279	-0.056342	4.580977
278.869455	7209.120763	14.751283	-0.056342	4.578518
278.995081	7201.140475	14.756288	-0.056360	4.576065
278.766130	7193.117834	14.761293	-0.056312	4.573597
278.676716	7185.138711	14.766298	-0.056290	4.571141
278.897881	7177.070618	14.771303	-0.056326	4.568656
278.605515	7169.074555	14.776307	-0.056266	4.566192
278.737700	7161.121789	14.781312	-0.056286	4.563740
278.540711	7153.091617	14.786317	-0.056244	4.561263
278.762734	7145.145017	14.791322	-0.056280	4.558811
278.587070	7137.159906	14.796327	-0.056242	4.556344
278.692640	7129.116274	14.801331	-0.056256	4.553859
278.608990	7121.107190	14.806336	-0.056235	4.551383
278.571055	7113.076042	14.811341	-0.056223	4.548899
278.537453	7105.116851	14.816346	-0.056212	4.546436
278.393220	7097.111187	14.821351	-0.056180	4.543957
278.465516	7089.105723	14.826355	-0.056188	4.541477
278.393760	7081.163844	14.831360	-0.056169	4.539015
278.412571	7073.125138	14.836365	-0.056167	4.536521
278.431168	7065.125049	14.841370	-0.056166	4.534039
278.162813	7057.072869	14.846375	-0.056110	4.531538
278.235333	7049.093335	14.851379	-0.056119	4.529059
278.239390	7041.115600	14.856384	-0.056114	4.526579
278.164196	7033.085592	14.861389	-0.056095	4.524082
278.200761	7025.146518	14.866394	-0.056097	4.521611
277.963373	7017.079461	14.871399	-0.056047	4.519099
278.123789	7009.107170	14.876403	-0.056072	4.516616
278.087964	7001.116692	14.881408	-0.056060	4.514125
277.772178	6993.000765	14.886413	-0.055996	4.511593
277.926240	6985.069749	14.891418	-0.056019	4.509119
277.856216	6977.029938	14.896423	-0.056001	4.506608
277.983258	6969.041922	14.901427	-0.056019	4.504113
277.932560	6961.071818	14.906432	-0.056005	4.501622
277.706497	6953.099730	14.911437	-0.055957	4.499128
277.698837	6945.086289	14.916442	-0.055951	4.496620
277.708689	6937.062214	14.921447	-0.055947	4.494108
277.638150	6929.027451	14.926451	-0.055929	4.491591
277.821692	6921.064475	14.931456	-0.055958	4.489095
277.666634	6913.045509	14.936461	-0.055924	4.486580
277.808223	6905.092778	14.941466	-0.055945	4.484085
277.538358	6897.083032	14.946471	-0.055889	4.481569
277.409334	6889.043643	14.951475	-0.055860	4.479043
277.677204	6881.082078	14.956480	-0.055905	4.476541
277.480745	6873.042563	14.961485	-0.055863	4.474012
277.369662	6865.019633	14.966490	-0.055837	4.471487
277.081030	6857.012199	14.971495	-0.055778	4.468965
277.272234	6849.000962	14.976499	-0.055808	4.466442
277.333064	6841.015500	14.981504	-0.055814	4.463925
277.078317	6833.035279	14.986509	-0.055762	4.461407
277.329831	6825.053604	14.991514	-0.055803	4.458889
277.307166	6817.038170	14.996519	-0.055794	4.456358
277.324352	6808.992238	15.001523	-0.055792	4.453816
277.208025	6801.037490	15.006528	-0.055765	4.451301
277.162102	6792.975875	15.011533	-0.055751	4.448751
277.117849	6785.020465	15.016538	-0.055738	4.446233
276.928941	6777.009395	15.021543	-0.055697	4.443695
277.020613	6769.044553	15.026547	-0.055709	4.441172
276.976394	6761.049622	15.031552	-0.055695	4.438637
276.842903	6753.006393	15.036557	-0.055665	4.436086
276.999971	6744.972657	15.041562	-0.055689	4.433536
276.836153	6736.949001	15.046567	-0.055654	4.430988
276.792223	6728.953858	15.051571	-0.055640	4.428447
276.803416	6721.010631	15.056576	-0.055637	4.425922
276.753422	6712.966880	15.061581	-0.055622	4.423362
276.712903	6705.000232	15.066586	-0.055610	4.420826
276.536263	6697.002014	15.071591	-0.055572	4.418278
276.563997	6688.966188	15.076595	-0.055571	4.415718
276.436457	6681.011816	15.081600	-0.055542	4.413181
276.372626	6672.924121	15.086605	-0.055525	4.410600
276.511947	6664.975824	15.091610	-0.055546	4.408063
276.523179	6656.931514	15.096615	-0.055543	4.405494
276.338459	6648.988835	15.101619	-0.055503	4.402955
276.406933	6641.012496	15.106624	-0.055511	4.400404
276.316593	6632.998535	15.111629	-0.055489	4.397839
276.450227	6625.028416	15.116634	-0.055508	4.395288
276.416228	6616.965383	15.121639	-0.055497	4.392705
276.243626	6608.951369	15.126643	-0.055459	4.390136
276.306787	6600.958456	15.131648	-0.055466	4.387572
276.335834	6592.959127	15.136653	-0.055466	4.385005
276.519241	6585.042407	15.141658	-0.055495	4.382464
276.388388	6576.994038	15.146663	-0.055465	4.379878
276.162007	6569.000763	15.151667	-0.055418	4.377307
275.989585	6561.002559	15.156672	-0.055381	4.374733
275.898333	6552.987267	15.161677	-0.055358	4.372153
276.101810	6544.957653	15.166682	-0.055391	4.369568
275.735465	6537.020037	15.171687	-0.055318	4.367008
275.970511	6528.938256	15.176691	-0.055356	4.364404
275.791166	6521.061745	15.181696	-0.055317	4.361861
275.602748	6512.992848	15.186701	-0.055277	4.359256
275.653776	6505.015927	15.191706	-0.055281	4.356679
275.865055	6496.965196	15.196711	-0.055315	4.354079
275.641435	6488.864254	15.201715	-0.055269	4.351457
275.682177	6480.914349	15.206720	-0.055271	4.348885
275.578628	6472.909442	15.211725	-0.055246	4.346293
275.744859	6464.967358	15.216730	-0.055272	4.343721
275.874918	6456.955577	15.221735	-0.055291	4.341124
275.676494	6448.961245	15.226739	-0.055249	4.338530
275.530780	6440.974508	15.231744	-0.055217	4.335937
275.500263	6432.949776	15.236749	-0.055206	4.333331
275.613381	6424.935424	15.241754	-0.055221	4.330727
275.390107	6416.952407	15.246759	-0.055175	4.328130
275.457144	6408.944851	15.251763	-0.055182	4.325525
275.536055	6401.003196	15.256768	-0.055191	4.322941
275.569269	6392.943688	15.261773	-0.055192	4.320316
275.573923	6385.019953	15.266778	-0.055188	4.317733
275.261821	6376.921578	15.271783	-0.055124	4.315090
275.491516	6368.916248	15.276787	-0.055162	4.312479
275.469325	6360.937780	15.281792	-0.055153	4.309874
275.239050	6352.919351	15.286797	-0.055104	4.307252
275.282171	6344.910906	15.291802	-0.055107	4.304635
275.094288	6337.011094	15.296807	-0.055067	4.302049
275.216943	6328.914146	15.301811	-0.055085	4.299400
275.117182	6320.972372	15.306816	-0.055061	4.296798
275.021342	6312.890603	15.311821	-0.055038	4.294148
274.909677	6304.891351	15.316826	-0.055012	4.291524
275.062929	6296.899993	15.321831	-0.055035	4.288903
275.129304	6288.894722	15.326835	-0.055042	4.286276
275.113996	6280.985699	15.331840	-0.055034	4.283677
274.769267	6272.935080	15.336845	-0.054965	4.281028
274.832020	6264.954143	15.341850	-0.054971	4.278403
274.782509	6256.959165	15.346855	-0.054957	4.275771
274.729929	6248.882979	15.351859	-0.054942	4.273111
274.561729	6240.876433	15.356864	-0.054905	4.270471
274.591617	6232.861181	15.361869	-0.054905	4.267828
274.652179	6224.869941	15.366874	-0.054911	4.265192
274.704675	6216.922598	15.371879	-0.054916	4.262569
274.572351	6208.875517	15.376883	-0.054886	4.259909
274.871860	6200.931344	15.381888	-0.054937	4.257286
274.577441	6192.923240	15.386893	-0.054876	4.254634
274.490331	6184.907015	15.391898	-0.054855	4.251980
274.502689	6176.878007	15.396903	-0.054852	4.249321
274.509081	6168.899400	15.401907	-0.054848	4.246677
274.393706	6160.942361	15.406912	-0.054821	4.244037
274.335777	6152.920039	15.411917	-0.054805	4.241375
274.439750	6144.988422	15.416922	-0.054819	4.238742
274.124247	6136.956283	15.421927	-0.054755	4.236071
274.084815	6128.903549	15.426931	-0.054743	4.233394
274.040076	6120.900185	15.431936	-0.054729	4.230731
273.965178	6112.905579	15.436941	-0.054710	4.228069
274.136015	6104.890077	15.441946	-0.054737	4.225401
273.951715	6096.932232	15.446951	-0.054697	4.222747
273.899883	6088.911886	15.451955	-0.054682	4.220072
273.832158	6080.993463	15.456960	-0.054664	4.217429
273.909842	6072.885911	15.461965	-0.054673	4.214722
273.947479	6064.924870	15.466970	-0.054675	4.212062
273.889294	6056.908304	15.471975	-0.054659	4.209382
273.670049	6048.927020	15.476979	-0.054613	4.206709
274.012296	6040.935382	15.481984	-0.054672	4.204037
273.593955	6032.973324	15.486989	-0.054588	4.201366
273.510404	6024.973423	15.491994	-0.054568	4.198683
273.454696	6016.960119	15.496999	-0.054552	4.195995
273.493869	6008.859700	15.502003	-0.054554	4.193277
273.639006	6000.828979	15.507008	-0.054576	4.190581
273.531959	5992.857911	15.512013	-0.054551	4.187901
273.466478	5984.889725	15.517018	-0.054533	4.185221
273.319893	5976.927460	15.522023	-0.054501	4.182540
273.322010	5968.905254	15.527027	-0.054496	4.179839
273.283335	5960.950720	15.532032	-0.054483	4.177158
273.162212	5952.906844	15.537037	-0.054456	4.174445
273.379648	5944.916192	15.542042	-0.054491	4.171752
273.477146	5936.888410	15.547047	-0.054504	4.169043
273.325185	5928.882529	15.552051	-0.054470	4.166337
273.130819	5920.948910	15.557056	-0.054429	4.163653
273.141891	5912.898159	15.562061	-0.054426	4.160930
273.323601	5904.912304	15.567066	-0.054454	4.158229
273.372271	5896.927860	15.572071	-0.054458	4.155525
273.102269	5888.882286	15.577075	-0.054402	4.152795
273.085514	5880.862747	15.582080	-0.054394	4.150075
273.088144	5872.873552	15.587085	-0.054389	4.147364
272.927746	5864.853052	15.592090	-0.054354	4.144639
272.803306	5856.956030	15.597095	-0.054326	4.141954
273.018719	5848.907060	15.602099	-0.054361	4.139220
272.793684	5840.925878	15.607104	-0.054314	4.136501
272.658596	5832.859723	15.612109	-0.054283	4.133753
272.790535	5824.849789	15.617114	-0.054302	4.131026
272.728287	5816.916245	15.622119	-0.054286	4.128320
272.661177	5808.874673	15.627123	-0.054268	4.125576
272.688502	5800.918208	15.632128	-0.054268	4.122860
272.684775	5792.904177	15.637133	-0.054262	4.120123
272.694277	5784.942466	15.642138	-0.054258	4.117401
272.748277	5776.894945	15.647143	-0.054263	4.114649
272.736096	5768.870779	15.652147	-0.054256	4.111902
272.436468	5760.876504	15.657152	-0.054195	4.109160
272.328704	5752.863117	15.662157	-0.054169	4.106412
272.396250	5744.874850	15.667162	-0.054177	4.103673
272.354006	5736.907016	15.672167	-0.054164	4.100938
272.174495	5728.943448	15.677171	-0.054125	4.098201
272.112365	5720.953495	15.682176	-0.054108	4.095454
272.259682	5712.906336	15.687181	-0.054130	4.092689
272.179167	5704.877098	15.692186	-0.054110	4.089924
272.188794	5696.902352	15.697191	-0.054107	4.087178
272.217689	5688.864283	15.702195	-0.054107	4.084409
272.328168	5680.975045	15.707200	-0.054122	4.081690
272.200636	5672.958514	15.712205	-0.054093	4.078922
272.125054	5664.957154	15.717210	-0.054074	4.076158
272.162844	5656.915148	15.722215	-0.054076	4.073380
272.037689	5648.900556	15.727219	-0.054047	4.070607
271.814151	5640.940582	15.732224	-0.054000	4.067849
271.721837	5632.884301	15.737229	-0.053978	4.065059
271.730396	5624.982586	15.742234	-0.053974	4.062321
271.963012	5616.943744	15.747239	-0.054012	4.059537
271.758810	5608.960801	15.752243	-0.053969	4.056764
271.905712	5600.949922	15.757248	-0.053991	4.053985
271.629923	5592.910951	15.762253	-0.053934	4.051188
271.653925	5584.945853	15.767258	-0.053934	4.048419
271.713133	5576.914746	15.772263	-0.053939	4.045626
271.597034	5568.992517	15.777267	-0.053913	4.042866
271.498617	5560.943316	15.782272	-0.053889	4.040060
271.539359	5552.941248	15.787277	-0.053891	4.037271
271.568362	5544.924630	15.792282	-0.053891	4.034475
271.468335	5536.819013	15.797287	-0.053868	4.031643
271.694987	5528.852372	15.802291	-0.053904	4.028864
271.678621	5520.893691	15.807296	-0.053896	4.026081
271.507597	5512.930342	15.812301	-0.053859	4.023292
271.440181	5504.938622	15.817306	-0.053841	4.020494
271.526387	5496.963541	15.822311	-0.053852	4.017701
271.248982	5488.914840	15.827315	-0.053795	4.014875
271.232129	5480.915484	15.832320	-0.053787	4.012068
271.235852	5472.898596	15.837325	-0.053782	4.009254
271.098904	5464.899879	15.842330	-0.053752	4.006441
270.897136	5456.932846	15.847335	-0.053709	4.003637
271.083108	5448.897152	15.852339	-0.053738	4.000813
271.236035	5440.953665	15.857344	-0.053761	3.998019
271.013343	5432.916787	15.862349	-0.053715	3.995184
270.883411	5424.934571	15.867354	-0.053685	3.992367
271.057709	5416.888308	15.872359	-0.053712	3.989531
270.750192	5408.894739	15.877363	-0.053650	3.986704
270.960418	5400.927975	15.882368	-0.053684	3.983893
271.013022	5392.942330	15.887373	-0.053688	3.981070
270.874050	5384.960721	15.892378	-0.053657	3.978244
270.547033	5376.931994	15.897383	-0.053591	3.975396
270.645984	5368.923401	15.902387	-0.053604	3.972560
270.681324	5360.907666	15.907392	-0.053606	3.969718
270.512756	5352.946070	15.912397	-0.053569	3.966890
270.576028	5344.943991	15.917402	-0.053576	3.964050
270.653585	5336.999638	15.922407	-0.053585	3.961228
270.275533	5328.986336	15.927411	-0.053509	3.958372
270.308424	5320.996812	15.932416	-0.053510	3.955529
270.481998	5312.902778	15.937421	-0.053537	3.952650
270.379071	5304.914760	15.942426	-0.053513	3.949801
270.184149	5296.952810	15.947431	-0.053471	3.946959
270.185994	5288.925802	15.952435	-0.053466	3.944094
270.471433	5280.997242	15.957440	-0.053514	3.941267
270.330965	5272.971364	15.962445	-0.053483	3.938396
270.279466	5264.990608	15.967450	-0.053468	3.935541
270.165736	5256.975184	15.972455	-0.053442	3.932670
270.011586	5248.951141	15.977459	-0.053408	3.929793
269.982752	5241.044277	15.982464	-0.053397	3.926958
269.982049	5232.989468	15.987469	-0.053392	3.924069
269.940021	5225.034848	15.992474	-0.053379	3.921212
269.894268	5217.051489	15.997479	-0.053365	3.918343
269.808804	5208.991827	16.002483	-0.053344	3.915444
270.044794	5200.991954	16.007488	-0.053382	3.912571
269.805969	5192.968568	16.012493	-0.053333	3.909677
269.677373	5185.031284	16.017498	-0.053303	3.906815
269.802920	5177.028705	16.022503	-0.053322	3.903932
269.677635	5168.991429	16.027507	-0.053293	3.901029
269.683520	5161.030257	16.032512	-0.053289	3.898155
269.718580	5152.989662	16.037517	-0.053290	3.895250
269.833992	5144.986210	16.042522	-0.053306	3.892357
269.593577	5136.967798	16.047527	-0.053256	3.889451
269.498633	5129.019293	16.052531	-0.053233	3.886570
269.585413	5121.052420	16.057536	-0.053244	3.883684
269.586145	5113.006555	16.062541	-0.053239	3.880766
269.556815	5105.031980	16.067546	-0.053229	3.877870
269.510610	5097.020476	16.072551	-0.053215	3.874959
269.403775	5088.771924	16.077555	-0.053189	3.871958
269.182618	5080.857677	16.082560	-0.053143	3.869075
269.156399	5072.884830	16.087565	-0.053133	3.866171
269.371111	5064.953661	16.092570	-0.053168	3.863285
269.328822	5056.968806	16.097575	-0.053155	3.860373
269.195001	5048.997599	16.102579	-0.053125	3.857461
269.220953	5040.984352	16.107584	-0.053124	3.854535
269.126552	5032.985555	16.112589	-0.053101	3.851610
268.974042	5024.994404	16.117594	-0.053068	3.848684
268.963700	5017.028760	16.122599	-0.053060	3.845768
269.075208	5009.010386	16.127603	-0.053076	3.842833
269.192154	5001.025032	16.132608	-0.053093	3.839908
268.934573	4993.068513	16.137613	-0.053039	3.836984
268.942634	4985.047066	16.142618	-0.053036	3.834039
268.969201	4977.045175	16.147623	-0.053035	3.831099
268.650404	4969.033428	16.152627	-0.052971	3.828146
268.972984	4961.039725	16.157632	-0.053026	3.825211
268.850105	4953.086018	16.162637	-0.052997	3.822279
268.687712	4945.044219	16.167642	-0.052962	3.819312
268.709486	4937.131802	16.172647	-0.052961	3.816394
268.826607	4929.059289	16.177651	-0.052977	3.813416
268.605356	4921.044783	16.182656	-0.052931	3.810451
268.473393	4913.044079	16.187661	-0.052901	3.807490
268.520555	4905.071243	16.192666	-0.052905	3.804541
268.646690	4897.140397	16.197671	-0.052923	3.801607
268.490463	4889.103394	16.202675	-0.052889	3.798625
268.473936	4881.123432	16.207680	-0.052880	3.795665
268.544509	4873.063834	16.212685	-0.052888	3.792675
268.425003	4865.036983	16.217690	-0.052861	3.789691
268.467921	4857.109247	16.222695	-0.052863	3.786745
268.479760	4849.056156	16.227699	-0.052860	3.783749
268.342446	4841.117295	16.232704	-0.052830	3.780790
268.188068	4833.106180	16.237709	-0.052796	3.777801
268.100236	4825.109176	16.242714	-0.052774	3.774817
268.083013	4817.110918	16.247719	-0.052765	3.771831
268.084883	4809.099467	16.252723	-0.052761	3.768839
268.001393	4801.127137	16.257728	-0.052740	3.765856
267.901130	4793.111307	16.262733	-0.052716	3.762855
267.814658	4785.115246	16.267738	-0.052695	3.759859
267.901571	4777.147412	16.272743	-0.052705	3.756876
267.758710	4769.101866	16.277747	-0.052674	3.753855
267.817724	4761.103579	16.282752	-0.052679	3.750855
267.535569	4753.109603	16.287757	-0.052622	3.747845
267.799672	4745.101420	16.292762	-0.052666	3.744841
267.881295	4737.140822	16.297767	-0.052676	3.741848
267.599310	4729.135599	16.302771	-0.052618	3.738827
267.641311	4721.148067	16.307776	-0.052620	3.735818
267.635326	4713.135232	16.312781	-0.052614	3.732796
267.765392	4705.091348	16.317786	-0.052633	3.729763
267.736342	4697.164018	16.322791	-0.052622	3.726768
267.623276	4689.153501	16.327795	-0.052596	3.723737
267.558233	4681.210004	16.332800	-0.052579	3.720729
267.256402	4673.253518	16.337805	-0.052517	3.717709
267.220985	4665.206645	16.342810	-0.052505	3.714659
267.384040	4657.116590	16.347815	-0.052530	3.711594
267.156462	4649.120879	16.352819	-0.052483	3.708553
267.349591	4641.128379	16.357824	-0.052514	3.705522
267.256568	4633.169976	16.362829	-0.052491	3.702493
267.215400	4625.186867	16.367834	-0.052478	3.699454
267.142747	4617.246816	16.372839	-0.052459	3.696428
267.155243	4609.185730	16.377843	-0.052456	3.693356
267.061279	4601.219342	16.382848	-0.052434	3.690315
267.041660	4593.217065	16.387853	-0.052425	3.687259
267.142385	4585.233073	16.392858	-0.052438	3.684210
267.030184	4577.267335	16.397863	-0.052412	3.681161
266.797538	4569.260014	16.402867	-0.052364	3.678090
266.777420	4561.265666	16.407872	-0.052355	3.675027
266.722870	4553.258327	16.412877	-0.052339	3.671956
266.640401	4545.233568	16.417882	-0.052319	3.668875
266.717415	4537.227606	16.422887	-0.052328	3.665802
266.695291	4529.244766	16.427891	-0.052318	3.662733
266.752621	4521.241349	16.432896	-0.052324	3.659656
266.561091	4513.290727	16.437901	-0.052283	3.656589
266.521345	4505.260400	16.442906	-0.052270	3.653494
266.789273	4497.252297	16.447911	-0.052315	3.650413
266.769746	4489.246280	16.452915	-0.052306	3.647322
266.599589	4481.267106	16.457920	-0.052269	3.644235
266.599546	4473.278213	16.462925	-0.052264	3.641146
266.498058	4465.298275	16.467930	-0.052240	3.638055
266.484441	4457.310218	16.472935	-0.052232	3.634961
266.293338	4449.259997	16.477939	-0.052191	3.631835
266.237200	4441.257265	16.482944	-0.052175	3.628729
266.282268	4433.239077	16.487949	-0.052179	3.625616
266.330697	4425.286140	16.492954	-0.052182	3.622527
266.627079	4417.284849	16.497959	-0.052232	3.619423
266.387031	4409.326477	16.502963	-0.052182	3.616318
266.237118	4401.327039	16.507968	-0.052149	3.613197
266.221344	4393.289078	16.512973	-0.052141	3.610062
266.149327	4385.346853	16.517978	-0.052122	3.606960
266.060589	4377.369554	16.522983	-0.052101	3.603841
265.886483	4369.373377	16.527987	-0.052063	3.600709
265.891052	4361.406533	16.532992	-0.052059	3.597592
266.168009	4353.371274	16.537997	-0.052105	3.594452
266.038299	4345.370597	16.543002	-0.052076	3.591312
266.016570	4337.372370	16.548007	-0.052066	3.588173
265.985588	4329.353219	16.553011	-0.052055	3.585023
265.957240	4321.419546	16.558016	-0.052045	3.581904
265.839602	4313.442977	16.563021	-0.052018	3.578763
265.790436	4305.416961	16.568026	-0.052003	3.575601
265.663044	4297.442593	16.573031	-0.051974	3.572455
265.547659	4289.398485	16.578035	-0.051948	3.569278
265.625876	4281.430354	16.583040	-0.051957	3.566135
265.437320	4273.431236	16.588045	-0.051917	3.562968
265.549934	4265.418637	16.593050	-0.051932	3.559803
265.633141	4257.476789	16.598055	-0.051943	3.556661
265.452394	4249.379596	16.603059	-0.051904	3.553448
265.367865	4241.344815	16.608064	-0.051883	3.550259
265.293917	4233.400629	16.613069	-0.051864	3.547104
265.180526	4225.400523	16.618074	-0.051837	3.543922
265.314314	4217.461301	16.623079	-0.051857	3.540769
265.174164	4209.449351	16.628083	-0.051826	3.537576
265.293900	4201.445460	16.633088	-0.051843	3.534391
265.141643	4193.441920	16.638093	-0.051809	3.531196
265.162173	4185.435720	16.643098	-0.051808	3.528001
265.199571	4177.468299	16.648103	-0.051809	3.524820
265.079491	4169.508356	16.653107	-0.051782	3.521634
265.073179	4161.529045	16.658112	-0.051775	3.518441
265.122098	4153.533276	16.663117	-0.051779	3.515240
265.006697	4145.501350	16.668122	-0.051752	3.512016
264.840339	4137.521999	16.673127	-0.051716	3.508809
264.733626	4129.500354	16.678131	-0.051691	3.505584
264.720459	4121.541006	16.683136	-0.051683	3.502384
264.805353	4113.521618	16.688141	-0.051694	3.499160
264.657720	4105.536972	16.693146	-0.051661	3.495940
264.837315	4097.571398	16.698151	-0.051690	3.492735
264.778783	4089.534224	16.703155	-0.051673	3.489490
264.716178	4081.575192	16.708160	-0.051656	3.486274
264.529878	4073.612412	16.713165	-0.051617	3.483049
264.515671	4065.613467	16.718170	-0.051609	3.479812
264.545538	4057.649317	16.723175	-0.051609	3.476588
264.313308	4049.605515	16.728179	-0.051561	3.473319
264.181922	4041.582162	16.733184	-0.051531	3.470060
264.228507	4033.602204	16.738189	-0.051534	3.466820
264.109358	4025.622942	16.743194	-0.051507	3.463573
264.490831	4017.592045	16.748199	-0.051573	3.460318
264.320565	4009.644146	16.753203	-0.051536	3.457075
264.254960	4001.644095	16.758208	-0.051518	3.453812
264.100950	3993.617461	16.763213	-0.051484	3.450531
264.106899	3985.638348	16.768218	-0.051480	3.447273
264.077569	3977.655895	16.773223	-0.051469	3.444008
264.098126	3969.664784	16.778227	-0.051468	3.440739
264.249561	3961.668343	16.783232	-0.051491	3.437469
264.115603	3953.691276	16.788237	-0.051461	3.434194
263.958346	3945.664478	16.793242	-0.051426	3.430894
264.127260	3937.681836	16.798247	-0.051453	3.427621
264.168140	3929.647428	16.803251	-0.051455	3.424319
263.956273	3921.743897	16.808256	-0.051410	3.421059
263.932178	3913.725721	16.813261	-0.051401	3.417755
263.829004	3905.725632	16.818266	-0.051376	3.414452
263.886032	3897.741238	16.823271	-0.051381	3.411159
263.636044	3889.733372	16.828275	-0.051330	3.407841
263.650844	3881.747613	16.833280	-0.051327	3.404539
263.643025	3873.794854	16.838285	-0.051320	3.401247
263.468551	3865.829092	16.843290	-0.051283	3.397940
263.475322	3857.816865	16.848295	-0.051279	3.394617
263.530386	3849.682165	16.853299	-0.051284	3.391241
263.531588	3841.749287	16.858304	-0.051279	3.387945
263.634794	3833.715016	16.863309	-0.051293	3.384606
263.500660	3825.803116	16.868314	-0.051263	3.381307
263.656504	3817.842241	16.873319	-0.051286	3.377994
263.569578	3809.788567	16.878323	-0.051265	3.374630
263.451636	3801.831531	16.883328	-0.051238	3.371303
263.466187	3793.841995	16.888333	-0.051235	3.367963
263.075403	3785.851050	16.893338	-0.051157	3.364605
263.069076	3777.920986	16.898343	-0.051151	3.361283
263.204204	3769.890620	16.903347	-0.051171	3.357921
263.072019	3761.886047	16.908352	-0.051141	3.354556
262.913556	3753.859162	16.913357	-0.051106	3.351178
262.935294	3745.844899	16.918362	-0.051105	3.347808
263.049969	3737.872151	16.923367	-0.051121	3.344456
262.876703	3729.913108	16.928371	-0.051084	3.341095
262.829311	3721.948982	16.933376	-0.051069	3.337734
263.078523	3713.913821	16.938381	-0.051111	3.334350
263.048629	3705.913326	16.943386	-0.051100	3.330967
262.869652	3697.946579	16.948391	-0.051061	3.327589
262.802160	3689.931807	16.953395	-0.051043	3.324192
262.725604	3681.976842	16.958400	-0.051024	3.320816
262.667680	3674.027628	16.963405	-0.051008	3.317440
262.776084	3665.990311	16.968410	-0.051023	3.314029
262.855725	3657.982111	16.973415	-0.051032	3.310626
262.544266	3649.977264	16.978419	-0.050969	3.307206
262.687751	3641.984292	16.983424	-0.050991	3.303805
262.600133	3634.031069	16.988429	-0.050969	3.300409
262.510867	3626.062114	16.993434	-0.050947	3.297002
262.687427	3618.073253	16.998439	-0.050975	3.293593
262.320870	3610.039258	17.003443	-0.050901	3.290141
262.449640	3602.058904	17.008448	-0.050920	3.286727
262.389426	3594.098000	17.013453	-0.050904	3.283311
262.306907	3586.095098	17.018458	-0.050883	3.279872
262.367894	3578.154440	17.023463	-0.050889	3.276462
262.067227	3570.112674	17.028467	-0.050828	3.272990
262.113323	3562.100226	17.033472	-0.050831	3.269541
262.086875	3554.140462	17.038477	-0.050821	3.266109
262.089290	3546.122821	17.043482	-0.050816	3.262649
262.140597	3538.163384	17.048487	-0.050821	3.259212
262.155788	3530.193266	17.053491	-0.050818	3.255765
261.998373	3522.173931	17.058496	-0.050784	3.252287
261.909561	3514.179977	17.063501	-0.050762	3.248819
261.854658	3506.198669	17.068506	-0.050747	3.245354
261.963801	3498.227269	17.073511	-0.050762	3.241896
261.924052	3490.227887	17.078515	-0.050749	3.238416
261.988392	3482.242516	17.083520	-0.050756	3.234943
262.034242	3474.187927	17.088525	-0.050759	3.231435
261.891497	3466.183971	17.093530	-0.050727	3.227938
261.581428	3458.245841	17.098535	-0.050664	3.224459
261.469908	3450.257872	17.103539	-0.050638	3.220962
261.574021	3442.286210	17.108544	-0.050652	3.217478
261.512707	3434.295244	17.113549	-0.050636	3.213974
261.563759	3426.273983	17.118554	-0.050640	3.210458
261.747166	3418.282394	17.123559	-0.050669	3.206957
261.492374	3410.322440	17.128563	-0.050616	3.203447
261.236391	3402.380669	17.133568	-0.050563	3.199942
261.455182	3394.392009	17.138573	-0.050599	3.196432
261.479640	3386.349151	17.143578	-0.050598	3.192886
261.305837	3378.363809	17.148583	-0.050561	3.189353
261.117492	3370.378911	17.153587	-0.050520	3.185816
261.148629	3362.403821	17.158592	-0.050521	3.182288
260.978741	3354.452624	17.163597	-0.050484	3.178759
260.898167	3346.440544	17.168602	-0.050464	3.175202
260.997579	3338.434905	17.173607	-0.050477	3.171652
260.986452	3330.416561	17.178611	-0.050470	3.168088
261.021361	3322.449077	17.183616	-0.050471	3.164544
261.052049	3314.482509	17.188621	-0.050471	3.160996
261.033398	3306.503075	17.193626	-0.050463	3.157437
260.621599	3298.542951	17.198631	-0.050381	3.153865
260.580094	3290.476372	17.203635	-0.050368	3.150258
260.801603	3282.519569	17.208640	-0.050404	3.146707
260.581355	3274.532695	17.213645	-0.050358	3.143119
260.556542	3266.540060	17.218650	-0.050348	3.139533
260.581658	3258.601003	17.223655	-0.050347	3.135969
260.448779	3250.577546	17.228659	-0.050317	3.132356
260.345198	3242.566763	17.233664	-0.050293	3.128746
260.445955	3234.610869	17.238669	-0.050306	3.125166
260.513771	3226.627881	17.243674	-0.050314	3.121568
260.474466	3218.681278	17.248679	-0.050301	3.117977
260.187713	3210.683571	17.253683	-0.050243	3.114348
260.268327	3202.651845	17.258688	-0.050252	3.110716
260.315519	3194.663091	17.263693	-0.050256	3.107098
260.193429	3186.670981	17.268698	-0.050228	3.103466
260.116260	3178.718819	17.273703	-0.050208	3.099850
260.122625	3170.747696	17.278707	-0.050204	3.096225
260.262928	3162.728579	17.283712	-0.050225	3.092580
260.151902	3154.748967	17.288717	-0.050199	3.088938
260.202266	3146.737237	17.293722	-0.050203	3.085283
260.147653	3138.800222	17.298727	-0.050188	3.081654
260.011881	3130.817385	17.303731	-0.050157	3.077996
260.133981	3122.796807	17.308736	-0.050175	3.074327
259.987449	3114.729385	17.313741	-0.050142	3.070621
259.790696	3106.781553	17.318746	-0.050100	3.066963
259.859635	3098.822280	17.323751	-0.050108	3.063307
259.878818	3090.811807	17.328755	-0.050106	3.059621
259.657081	3082.891199	17.333760	-0.050060	3.055961
259.479286	3074.908730	17.338765	-0.050022	3.052270
259.538714	3066.874448	17.343770	-0.050027	3.048562
259.481441	3058.911869	17.348775	-0.050012	3.044876
259.241269	3050.973809	17.353779	-0.049962	3.041189
259.310259	3042.977166	17.358784	-0.049969	3.037485
259.598911	3034.968816	17.363789	-0.050018	3.033782
259.358411	3026.959936	17.368794	-0.049968	3.030048
259.512984	3018.987667	17.373799	-0.049991	3.026346
259.342518	3011.022126	17.378803	-0.049954	3.022627
259.296961	3003.035373	17.383808	-0.049941	3.018899
259.173687	2995.082008	17.388813	-0.049912	3.015179
259.179747	2987.063581	17.393818	-0.049908	3.011430
259.114344	2979.073306	17.398823	-0.049891	3.007686
258.983304	2971.093266	17.403827	-0.049861	3.003938
259.012418	2963.112356	17.408832	-0.049861	3.000194
259.058591	2955.167478	17.413837	-0.049865	2.996462
258.858582	2947.124578	17.418842	-0.049822	2.992668
258.770662	2939.160234	17.423847	-0.049801	2.988911
258.759231	2931.138965	17.428851	-0.049793	2.985127
258.742788	2923.179932	17.433856	-0.049785	2.981366
258.634793	2915.232789	17.438861	-0.049760	2.977603
258.730934	2907.203459	17.443866	-0.049772	2.973805
258.947826	2899.210904	17.448871	-0.049808	2.970027
258.709122	2891.257507	17.453875	-0.049758	2.966239
258.779758	2883.277253	17.458880	-0.049766	2.962449
258.779783	2875.306247	17.463885	-0.049761	2.958655
258.382170	2867.350330	17.468890	-0.049681	2.954843
258.644474	2859.317328	17.473895	-0.049725	2.951023
258.780595	2851.325209	17.478899	-0.049745	2.947212
258.652702	2843.366735	17.483904	-0.049716	2.943398
258.226147	2835.438674	17.488909	-0.049631	2.939577
258.314357	2827.437227	17.493914	-0.049643	2.935744
258.551175	2819.417664	17.498919	-0.049681	2.931905
258.356490	2811.440626	17.503923	-0.049640	2.928058
258.411209	2803.449514	17.508928	-0.049645	2.924213
258.440160	2795.492412	17.513933	-0.049645	2.920377
258.164619	2787.547473	17.518938	-0.049588	2.916526
257.971384	2779.515081	17.523943	-0.049547	2.912633
258.192862	2771.447255	17.528947	-0.049583	2.908739
258.127630	2763.482860	17.533952	-0.049566	2.904874
257.988221	2755.566212	17.538957	-0.049535	2.901024
257.967331	2747.582852	17.543962	-0.049526	2.897142
258.022898	2739.588911	17.548967	-0.049531	2.893254
257.699452	2731.602948	17.553971	-0.049465	2.889345
257.750665	2723.640645	17.558976	-0.049470	2.885462
257.918508	2715.664550	17.563981	-0.049496	2.881573
257.790468	2707.695809	17.568986	-0.049466	2.877666
257.662104	2699.729717	17.573991	-0.049437	2.873756
257.592405	2691.701845	17.578995	-0.049419	2.869813
257.595576	2683.737825	17.584000	-0.049414	2.865899
257.652091	2675.779955	17.589005	-0.049420	2.861987
257.482207	2667.797631	17.594010	-0.049383	2.858044
257.643777	2659.809911	17.599015	-0.049408	2.854112
257.337294	2651.835455	17.604019	-0.049345	2.850155
257.415591	2643.836909	17.609024	-0.049355	2.846202
257.417776	2635.892691	17.614029	-0.049350	2.842266
257.394214	2627.908948	17.619034	-0.049340	2.838304
257.425130	2619.944616	17.624039	-0.049341	2.834348
257.251417	2611.926277	17.629043	-0.049303	2.830349
257.129833	2603.954118	17.634048	-0.049275	2.826370
257.203573	2595.977808	17.639053	-0.049284	2.822395
257.201881	2587.988238	17.644058	-0.049278	2.818403
257.263759	2580.017663	17.649063	-0.049285	2.814418
257.206070	2572.016662	17.654067	-0.049269	2.810406
256.997333	2564.071853	17.659072	-0.049225	2.806407
256.865935	2556.127085	17.664077	-0.049195	2.802407
256.833066	2548.137720	17.669082	-0.049184	2.798385
256.899410	2540.163865	17.674087	-0.049191	2.794370
256.957072	2532.132584	17.679091	-0.049196	2.790320
256.964366	2524.150872	17.684096	-0.049192	2.786287
256.972947	2516.183029	17.689101	-0.049189	2.782254
256.682385	2508.248012	17.694106	-0.049129	2.778215
256.645970	2500.284001	17.699111	-0.049117	2.774170
256.611336	2492.260230	17.704115	-0.049106	2.770089
256.431525	2484.322272	17.709120	-0.049067	2.766037
256.510008	2476.345587	17.714125	-0.049076	2.761975
256.543248	2468.353522	17.719130	-0.049077	2.757896
256.437795	2460.383465	17.724135	-0.049053	2.753814
256.219355	2452.336861	17.729139	-0.049007	2.749679
256.273203	2444.370113	17.734144	-0.049011	2.745597
256.411058	2436.413763	17.739149	-0.049032	2.741518
256.175013	2428.457021	17.744154	-0.048983	2.737410
256.165592	2420.475198	17.749159	-0.048976	2.733297
255.973795	2412.503466	17.754163	-0.048935	2.729172
256.144543	2404.513460	17.759168	-0.048961	2.725054
256.054229	2396.574364	17.764173	-0.048939	2.720939
256.149899	2388.597454	17.769178	-0.048952	2.716810
256.002714	2380.619567	17.774183	-0.048919	2.712660
255.968331	2372.606272	17.779187	-0.048908	2.708491
256.053397	2364.627555	17.784192	-0.048918	2.704342
256.143224	2356.665846	17.789197	-0.048930	2.700195
255.890090	2348.733669	17.794202	-0.048877	2.696036
255.685342	2340.764514	17.799207	-0.048834	2.691854
255.843036	2332.768895	17.804211	-0.048858	2.687675
255.504172	2324.831950	17.809216	-0.048790	2.683488
255.545427	2316.877603	17.814221	-0.048792	2.679310
255.634301	2308.881272	17.819226	-0.048804	2.675106
255.349194	2300.899672	17.824231	-0.048745	2.670879
255.147095	2292.914868	17.829235	-0.048702	2.666650
255.373784	2284.907722	17.834240	-0.048739	2.662429
255.328923	2276.953922	17.839245	-0.048726	2.658213
255.148437	2268.991711	17.844250	-0.048687	2.653976
255.264444	2260.982846	17.849255	-0.048703	2.649727
255.304688	2253.032962	17.854259	-0.048706	2.645498
255.079940	2245.089680	17.859264	-0.048659	2.641248
255.219814	2237.117983	17.864269	-0.048679	2.637000
255.161422	2229.115520	17.869274	-0.048663	2.632716
255.287788	2221.133311	17.874279	-0.048682	2.628448
254.927922	2213.193830	17.879283	-0.048609	2.624163
254.902630	2205.218003	17.884288	-0.048599	2.619874
254.990863	2197.277391	17.889293	-0.048611	2.615605
254.992571	2189.259778	17.894298	-0.048606	2.611281
255.031335	2181.306272	17.899303	-0.048608	2.606988
254.922661	2173.343264	17.904307	-0.048582	2.602672
254.643305	2165.425167	17.909312	-0.048525	2.598361
254.633729	2157.420312	17.914317	-0.048518	2.594015
254.692408	2149.233620	17.919322	-0.048524	2.589567
254.643755	2141.315485	17.924327	-0.048509	2.585251
254.548951	2133.394379	17.929331	-0.048487	2.580922
254.649418	2125.438960	17.934336	-0.048500	2.576581
254.479728	2117.506099	17.939341	-0.048463	2.572226
254.284344	2109.541375	17.944346	-0.048422	2.567845
254.307059	2101.584686	17.949351	-0.048421	2.563476
254.333967	2093.635347	17.954355	-0.048420	2.559103
254.428716	2085.651937	17.959360	-0.048433	2.554709
254.409073	2077.671568	17.964365	-0.048424	2.550301
254.233777	2069.716030	17.969370	-0.048386	2.545888
254.050552	2061.802698	17.974375	-0.048347	2.541491
254.003033	2053.830246	17.979379	-0.048333	2.537062
253.975677	2045.845323	17.984384	-0.048322	2.532620
253.986256	2037.875453	17.989389	-0.048319	2.528182
254.022471	2029.894205	17.994394	-0.048321	2.523731
253.905825	2021.963340	17.999399	-0.048294	2.519289
253.673176	2014.024373	18.004403	-0.048245	2.514827
253.624290	2006.000669	18.009408	-0.048231	2.510322
253.647634	1998.028992	18.014413	-0.048230	2.505844
253.696184	1990.048905	18.019418	-0.048234	2.501355
253.712345	1982.115771	18.024423	-0.048232	2.496882
253.575786	1974.155859	18.029427	-0.048201	2.492375
253.339180	1966.187012	18.034432	-0.048152	2.487847
253.341776	1958.237542	18.039437	-0.048147	2.483339
253.085523	1950.290823	18.044442	-0.048094	2.478805
253.266661	1942.318613	18.049447	-0.048123	2.474282
253.295213	1934.303610	18.054451	-0.048123	2.469714
253.070364	1926.366503	18.059456	-0.048076	2.465163
253.081468	1918.418806	18.064461	-0.048072	2.460615
252.907181	1910.459455	18.069466	-0.048035	2.456038
252.836126	1902.512102	18.074471	-0.048016	2.451468
252.761775	1894.533432	18.079475	-0.047997	2.446870
252.844824	1886.562093	18.084480	-0.048007	2.442280
253.078725	1878.597431	18.089485	-0.048046	2.437697
252.690543	1870.649027	18.094490	-0.047968	2.433067
252.855431	1862.626576	18.099495	-0.047994	2.428428
252.719919	1854.674356	18.104499	-0.047963	2.423797
252.588559	1846.740880	18.109504	-0.047934	2.419169
252.683246	1838.782798	18.114509	-0.047946	2.414535
252.748804	1830.778673	18.119514	-0.047953	2.409863
252.617471	1822.852426	18.124519	-0.047923	2.405212
252.545185	1814.919899	18.129523	-0.047905	2.400553
252.464758	1806.970728	18.134528	-0.047884	2.395875
252.439809	1799.009064	18.139533	-0.047875	2.391184
252.226494	1791.047786	18.144538	-0.047830	2.386469
252.122634	1783.101688	18.149543	-0.047805	2.381763
252.216044	1775.134103	18.154547	-0.047817	2.377050
252.052016	1767.177945	18.159552	-0.047782	2.372315
252.001781	1759.217746	18.164557	-0.047767	2.367576
251.962253	1751.259766	18.169562	-0.047754	2.362830
252.171903	1743.300369	18.174567	-0.047788	2.358094
251.933553	1735.358436	18.179571	-0.047739	2.353322
251.816831	1727.374431	18.184576	-0.047712	2.348526
251.888086	1719.419492	18.189581	-0.047720	2.343752
251.654514	1711.489420	18.194586	-0.047671	2.338959
251.631158	1703.529354	18.199591	-0.047661	2.334155
251.654123	1695.561322	18.204595	-0.047661	2.329340
251.495183	1687.610841	18.209600	-0.047626	2.324510
251.664345	1679.662268	18.214605	-0.047652	2.319699
251.656548	1671.710661	18.219610	-0.047645	2.314861
251.742391	1663.719370	18.224615	-0.047656	2.309997
251.555502	1655.782720	18.229619	-0.047616	2.305133
251.386198	1647.859249	18.234624	-0.047579	2.300268
251.381580	1639.927219	18.239629	-0.047573	2.295402
251.379415	1631.931005	18.244634	-0.047568	2.290486
251.457517	1623.988218	18.249639	-0.047577	2.285599
251.524423	1616.033085	18.254643	-0.047584	2.280693
251.424737	1608.107192	18.259648	-0.047561	2.275781
251.197483	1600.116034	18.264653	-0.047513	2.270806
251.127850	1592.136751	18.269658	-0.047495	2.265841
251.302723	1584.188138	18.274663	-0.047522	2.260906
251.267922	1576.256899	18.279667	-0.047510	2.255952
251.263377	1568.289278	18.284672	-0.047504	2.250967
251.215889	1560.352739	18.289677	-0.047490	2.245988
251.022258	1552.441056	18.294682	-0.047449	2.240999
250.910723	1544.524498	18.299687	-0.047423	2.236004
250.963967	1536.543106	18.304691	-0.047428	2.230971
250.978961	1528.569501	18.309696	-0.047425	2.225929
250.894564	1520.653950	18.314701	-0.047404	2.220903
250.547432	1512.736341	18.319706	-0.047335	2.215840
250.755735	1504.749872	18.324711	-0.047368	2.210772
250.644528	1496.814834	18.329715	-0.047342	2.205697
250.455354	1488.894499	18.334720	-0.047302	2.200612
250.556858	1480.949834	18.339725	-0.047316	2.195526
250.458920	1472.958558	18.344730	-0.047292	2.190380
250.293557	1465.031961	18.349735	-0.047256	2.185257
250.195673	1457.100240	18.354739	-0.047233	2.180125
250.302236	1449.154604	18.359744	-0.047247	2.174991
250.446710	1441.171308	18.364749	-0.047269	2.169824
250.266728	1433.252147	18.369754	-0.047230	2.164656
250.192663	1425.341213	18.374759	-0.047211	2.159491
250.370642	1417.388449	18.379763	-0.047239	2.154310
250.105871	1409.435390	18.384768	-0.047185	2.149074
250.135920	1401.501463	18.389773	-0.047185	2.143866
250.126723	1393.568009	18.394778	-0.047178	2.138642
249.973233	1385.655032	18.399783	-0.047144	2.133405
249.922524	1377.702977	18.404787	-0.047130	2.128139
249.881667	1369.765443	18.409792	-0.047117	2.122871
249.974093	1361.839673	18.414797	-0.047129	2.117610
249.828718	1353.868422	18.419802	-0.047097	2.112282
249.741979	1345.910997	18.424807	-0.047075	2.106956
249.714392	1337.984726	18.429811	-0.047065	2.101643
249.754313	1330.037382	18.434816	-0.047067	2.096309
249.623098	1322.129948	18.439821	-0.047038	2.090972
249.803909	1314.146420	18.444826	-0.047066	2.085600
249.757198	1306.242194	18.449831	-0.047052	2.080246
249.670798	1298.345274	18.454835	-0.047031	2.074879
249.592115	1290.391630	18.459840	-0.047011	2.069460
249.603171	1282.457636	18.464845	-0.047008	2.064049
249.261435	1274.585060	18.469850	-0.046939	2.058630
249.236239	1266.649367	18.474855	-0.046929	2.053186
249.428706	1258.659049	18.479859	-0.046960	2.047711
248.982683	1250.799030	18.484864	-0.046872	2.042248
249.122790	1242.873086	18.489869	-0.046892	2.036783
248.943417	1234.922188	18.494874	-0.046854	2.031254
248.915780	1226.980114	18.499879	-0.046844	2.025731
248.844704	1219.053803	18.504883	-0.046825	2.020200
248.838983	1211.129982	18.509888	-0.046819	2.014662
248.749779	1203.210914	18.514893	-0.046797	2.009103
248.688643	1195.273712	18.519898	-0.046780	2.003520
248.481478	1187.396690	18.524903	-0.046737	1.997947
248.558862	1179.441945	18.529907	-0.046746	1.992334
248.258477	1171.536451	18.534912	-0.046685	1.986700
248.481195	1163.586014	18.539917	-0.046721	1.981074
248.597658	1155.641427	18.544922	-0.046738	1.975424
248.803546	1147.686249	18.549927	-0.046771	1.969761
248.468747	1139.830226	18.554931	-0.046703	1.964094
248.377636	1131.924436	18.559936	-0.046681	1.958401
248.204524	1124.018511	18.564941	-0.046644	1.952682
248.041226	1116.055921	18.569946	-0.046608	1.946907
248.064815	1108.134118	18.574951	-0.046607	1.941164
248.094456	1100.234582	18.579955	-0.046608	1.935421
247.978797	1092.306186	18.584960	-0.046581	1.929624
247.973407	1084.392718	18.589965	-0.046575	1.923833
247.697682	1076.522638	18.594970	-0.046518	1.918026
247.663538	1068.591159	18.599975	-0.046507	1.912183
247.731549	1060.657055	18.604979	-0.046514	1.906332
247.793612	1052.730868	18.609984	-0.046520	1.900468
247.845728	1044.832456	18.614989	-0.046525	1.894605
247.587155	1036.934739	18.619994	-0.046472	1.888689
247.483283	1029.051755	18.624999	-0.046447	1.882783
247.565640	1021.135888	18.630003	-0.046457	1.876856
247.255873	1013.238866	18.635008	-0.046394	1.870878
247.335087	1005.300267	18.640013	-0.046404	1.864895
247.362142	997.391309	18.645018	-0.046404	1.858909
247.444125	989.477405	18.650023	-0.046414	1.852906
247.403762	981.578348	18.655027	-0.046401	1.846881
247.231901	973.689377	18.660032	-0.046364	1.840829
247.150946	965.823464	18.665037	-0.046344	1.834784
247.093540	957.891202	18.670042	-0.046328	1.828672
246.952550	950.014693	18.675047	-0.046296	1.822572
247.073096	942.108408	18.680051	-0.046314	1.816460
246.821695	934.227506	18.685056	-0.046262	1.810302
246.728436	926.336567	18.690061	-0.046239	1.804134
246.816919	918.436751	18.695066	-0.046250	1.797960
246.862904	910.501103	18.700071	-0.046254	1.791732
246.697755	902.595686	18.705075	-0.046218	1.785480
246.515897	894.733465	18.710080	-0.046179	1.779238
246.492563	886.849561	18.715085	-0.046169	1.772976
246.602473	878.920699	18.720090	-0.046185	1.766673
246.400651	871.081273	18.725095	-0.046142	1.760380
246.378976	863.195088	18.730099	-0.046133	1.754049
246.379754	855.270759	18.735104	-0.046128	1.747668
246.298528	847.414955	18.740109	-0.046107	1.741308
246.318279	839.534214	18.745114	-0.046106	1.734917
246.289925	831.647507	18.750119	-0.046095	1.728492
246.045706	823.802854	18.755123	-0.046045	1.722050
245.889280	815.950189	18.760128	-0.046011	1.715588
246.022508	808.028424	18.765133	-0.046030	1.709082
245.870730	800.150289	18.770138	-0.045997	1.702550
245.799437	792.293342	18.775143	-0.045978	1.696021
245.772357	784.409175	18.780147	-0.045968	1.689450
245.572621	776.550186	18.785152	-0.045926	1.682851
245.710486	768.680918	18.790157	-0.045946	1.676263
245.627371	760.795932	18.795162	-0.045926	1.669606
245.721596	752.910016	18.800167	-0.045938	1.662945
245.603213	745.071194	18.805171	-0.045911	1.656269
245.273014	737.240782	18.810176	-0.045844	1.649545
245.316401	729.373573	18.815181	-0.045847	1.642812
245.135000	721.537974	18.820186	-0.045808	1.636047
245.253492	713.597709	18.825191	-0.045825	1.629206
245.279059	705.724327	18.830195	-0.045825	1.622381
245.364883	697.858414	18.835200	-0.045836	1.615542
245.127534	690.049330	18.840205	-0.045786	1.608678
244.792440	682.240331	18.845210	-0.045719	1.601771
244.846858	674.387689	18.850215	-0.045724	1.594851
244.772480	666.528727	18.855219	-0.045705	1.587876
244.671288	658.688668	18.860224	-0.045681	1.580884
244.767390	650.835479	18.865229	-0.045693	1.573877
244.707587	642.981719	18.870234	-0.045677	1.566816
244.483338	635.179922	18.875239	-0.045630	1.559746
244.572402	627.323939	18.880243	-0.045642	1.552641
244.375067	619.482397	18.885248	-0.045600	1.545473
244.314190	611.681116	18.890253	-0.045583	1.538330
244.124170	603.845337	18.895258	-0.045543	1.531102
244.269541	595.987425	18.900263	-0.045565	1.523869
244.294479	588.174082	18.905267	-0.045564	1.516626
243.950783	580.374997	18.910272	-0.045495	1.509304
243.812460	572.574729	18.915277	-0.045464	1.501978
243.767640	564.751485	18.920282	-0.045451	1.494608
243.850543	556.904080	18.925287	-0.045461	1.487198
243.894927	549.096325	18.930291	-0.045464	1.479783
243.725124	541.285576	18.935296	-0.045428	1.472295
243.523278	533.475665	18.940301	-0.045385	1.464763
243.357911	525.692327	18.945306	-0.045349	1.457224
243.566257	517.835892	18.950311	-0.045383	1.449635
243.419061	510.070651	18.955315	-0.045350	1.442037
243.242572	502.298680	18.960320	-0.045312	1.434388
243.367042	494.469320	18.965325	-0.045330	1.426691
243.261863	486.697906	18.970330	-0.045306	1.418971
243.164491	478.911584	18.975335	-0.045282	1.411196
243.000927	471.159726	18.980339	-0.045247	1.403400
242.839131	463.396511	18.985344	-0.045212	1.395551
242.825310	455.601654	18.990349	-0.045204	1.387649
242.556425	447.858196	18.995354	-0.045149	1.379712
242.653242	440.054796	19.000359	-0.045162	1.371729
242.567171	432.295924	19.005363	-0.045141	1.363714
242.465067	424.544203	19.010368	-0.045116	1.355657
242.598245	416.749317	19.015373	-0.045136	1.347547
242.490408	409.011364	19.020378	-0.045111	1.339405
242.393042	401.268315	19.025383	-0.045088	1.331211
242.162729	393.559982	19.030387	-0.045040	1.322978
242.055373	385.804237	19.035392	-0.045015	1.314666
242.016441	377.945801	19.040397	-0.045002	1.306201
241.754584	370.260197	19.045402	-0.044949	1.297829
241.884234	362.499940	19.050407	-0.044968	1.289393
241.704477	354.816000	19.055411	-0.044929	1.280928
241.710939	347.094366	19.060416	-0.044925	1.272399
241.774511	339.365922	19.065421	-0.044932	1.263816
241.562846	331.696552	19.070426	-0.044888	1.255188
241.469730	323.996663	19.075431	-0.044865	1.246489
241.474854	316.312740	19.080435	-0.044861	1.237766
241.377153	308.605540	19.085440	-0.044838	1.228934
241.302012	300.927584	19.090445	-0.044819	1.220076
241.190894	293.258725	19.095450	-0.044793	1.211157
241.002334	285.612392	19.100455	-0.044753	1.202183
241.152845	277.925086	19.105459	-0.044776	1.193161
240.818801	270.294709	19.110464	-0.044709	1.184040
240.708548	262.663479	19.115469	-0.044683	1.174892
240.728542	254.997575	19.120474	-0.044682	1.165658
240.566836	247.388529	19.125479	-0.044647	1.156381
240.443235	239.723149	19.130483	-0.044619	1.146968
240.257992	232.117115	19.135488	-0.044579	1.137538
240.534845	224.448348	19.140493	-0.044626	1.128049
240.202628	216.895157	19.145498	-0.044559	1.118494
240.166491	209.285899	19.150503	-0.044547	1.108849
240.143942	201.693923	19.155507	-0.044538	1.099146
239.973272	194.123480	19.160512	-0.044501	1.089350
239.911205	186.564888	19.165517	-0.044485	1.079506
239.701856	179.019622	19.170522	-0.044441	1.069555
239.724417	171.443872	19.175527	-0.044440	1.059523
239.609105	163.917807	19.180531	-0.044414	1.049430
239.538229	156.383338	19.185536	-0.044396	1.039238
239.549828	148.855751	19.190541	-0.044393	1.028974
239.195811	141.400610	19.195546	-0.044322	1.018618
238.923023	133.933813	19.200551	-0.044266	1.008160
239.006228	126.434375	19.205555	-0.044277	0.997634
238.832295	118.935203	19.210560	-0.044240	0.986931
238.789236	111.477481	19.215565	-0.044227	0.976204
238.528861	104.056966	19.220570	-0.044173	0.965357
238.379554	96.647966	19.225575	-0.044141	0.954432
238.353227	89.222216	19.230579	-0.044131	0.943388
238.215923	81.827074	19.235584	-0.044101	0.932229
238.202177	74.444642	19.240589	-0.044093	0.920988
237.854561	67.121831	19.245594	-0.044024	0.909610
237.873911	59.984391	19.250599	-0.044023	0.898479