Fri Mar 12 11:55:17 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.647023	-0.009627	0.000000	-0.000013	0.720969
0.621846	-0.056277	0.005005	-0.000009	0.720869
0.689310	-0.063853	0.010010	-0.000021	0.720877
0.781222	-0.083001	0.015014	-0.000038	0.720872
0.716524	-0.071682	0.020019	-0.000026	0.720872
0.800841	-0.083131	0.025024	-0.000042	0.720879
0.585104	-0.051262	0.030029	-0.000002	0.720866
0.513262	-0.035617	0.035034	0.000012	0.720871
0.784490	-0.083326	0.040038	-0.000039	0.720873
0.765063	-0.081457	0.045043	-0.000035	0.720869
0.694014	-0.064843	0.050048	-0.000022	0.720877
0.938723	-0.111795	0.055053	-0.000068	0.720871
0.933908	-0.108761	0.060058	-0.000067	0.720875
0.829724	-0.092076	0.065062	-0.000047	0.720871
0.902436	-0.190851	0.070067	-0.000061	0.720702
0.887921	-0.272052	0.075072	-0.000058	0.720537
0.870462	-0.273506	0.080077	-0.000055	0.720528
0.795394	-0.254909	0.085082	-0.000041	0.720539
0.830311	-0.260219	0.090086	-0.000047	0.720540
0.808081	-0.259159	0.095091	-0.000043	0.720535
0.712401	-0.278635	0.100096	-0.000025	0.720463
0.601123	-0.383315	0.105101	-0.000005	0.720218
0.749794	-0.406466	0.110106	-0.000032	0.720224
0.785043	-0.413897	0.115110	-0.000039	0.720222
0.464758	-0.358607	0.120115	0.000021	0.720219
0.605007	-0.391037	0.125120	-0.000005	0.720204
0.549525	-0.538803	0.130125	0.000005	0.719893
0.670638	-0.558158	0.135130	-0.000017	0.719898
0.650051	-0.555050	0.140134	-0.000014	0.719897
0.850178	-0.591724	0.145139	-0.000051	0.719895
0.889166	-0.718552	0.150144	-0.000058	0.719658
0.678162	-0.713407	0.155149	-0.000019	0.719594
0.742830	-0.721919	0.160154	-0.000031	0.719600
0.732386	-0.743304	0.165158	-0.000029	0.719555
0.586434	-0.864723	0.170163	-0.000002	0.719264
0.735393	-0.884964	0.175168	-0.000029	0.719276
0.838385	-0.908456	0.180173	-0.000049	0.719266
0.701748	-1.009597	0.185178	-0.000023	0.719019
0.448237	-0.993924	0.190182	0.000024	0.718961
0.536025	-1.013044	0.195187	0.000008	0.718954
0.643739	-1.127239	0.200192	-0.000012	0.718766
0.653544	-1.192774	0.205197	-0.000014	0.718640
0.566623	-1.175676	0.210202	0.000002	0.718643
0.531541	-1.275031	0.215206	0.000009	0.718435
0.407638	-1.296447	0.220211	0.000032	0.718349
0.579561	-1.324305	0.225216	-0.000000	0.718355
0.369791	-1.449715	0.230221	0.000039	0.718033
0.408966	-1.465507	0.235226	0.000032	0.718016
0.397272	-1.504789	0.240230	0.000034	0.717934
0.581576	-1.657015	0.245235	-0.000000	0.717698
0.418199	-1.624287	0.250240	0.000030	0.717705
0.465053	-1.760441	0.255245	0.000021	0.717453
0.410643	-1.789793	0.260250	0.000032	0.717375
0.192534	-1.804308	0.265254	0.000072	0.717270
-0.069906	-1.855544	0.270259	0.000121	0.717076
0.262441	-1.911197	0.275264	0.000059	0.717083
0.179012	-2.058030	0.280269	0.000075	0.716763
0.147988	-2.055702	0.285274	0.000081	0.716757
-0.165422	-2.104529	0.290278	0.000139	0.716550
-0.157358	-2.159308	0.295283	0.000138	0.716444
-0.308715	-2.186784	0.300288	0.000166	0.716336
-0.540952	-2.250834	0.305293	0.000209	0.716128
-0.344573	-2.294765	0.310298	0.000173	0.716110
-1.837368	-2.142144	0.315302	0.000450	0.715885
-2.249709	-2.070506	0.320307	0.000527	0.715882
-2.259500	-2.113624	0.325312	0.000529	0.715793
-3.171633	-2.077571	0.330317	0.000699	0.715542
-2.909775	-2.122373	0.335322	0.000650	0.715546
-3.150014	-2.097925	0.340326	0.000695	0.715510
-3.959111	-2.097996	0.345331	0.000845	0.715224
-3.768035	-2.125508	0.350336	0.000810	0.715237
-4.279838	-2.038035	0.355341	0.000905	0.715229
-3.958375	-2.196104	0.360346	0.000845	0.715029
-5.057483	-2.061703	0.365350	0.001050	0.714907
-5.068993	-2.063826	0.370355	0.001052	0.714899
-4.514196	-2.157751	0.375360	0.000949	0.714909
-5.507449	-2.092761	0.380365	0.001134	0.714687
-6.223062	-2.006203	0.385370	0.001267	0.714605
-5.521634	-2.130777	0.390374	0.001136	0.714606
-5.922525	-2.064156	0.395379	0.001211	0.714597
-6.120733	-2.054597	0.400384	0.001248	0.714546
-6.724557	-2.085878	0.405389	0.001360	0.714270
-6.494175	-2.126455	0.410394	0.001317	0.714271
-6.975298	-2.037324	0.415398	0.001407	0.714278
-6.877934	-2.058408	0.420403	0.001389	0.714270
-6.370554	-2.192459	0.425408	0.001294	0.714183
-8.083385	-1.996783	0.430413	0.001613	0.713966
-7.635291	-2.074814	0.435418	0.001530	0.713969
-7.610875	-2.078422	0.440422	0.001525	0.713971
-7.879647	-2.033644	0.445427	0.001575	0.713965
-7.705771	-2.061013	0.450432	0.001543	0.713972
-8.094421	-2.131804	0.455437	0.001615	0.713694
-8.561586	-2.069461	0.460442	0.001702	0.713652
-8.838200	-2.019240	0.465446	0.001754	0.713654
-8.807974	-2.028712	0.470451	0.001748	0.713646
-8.477030	-2.083047	0.475456	0.001687	0.713655
-8.737196	-2.039957	0.480461	0.001735	0.713649
-9.423041	-2.060123	0.485466	0.001863	0.713365
-9.134131	-2.113799	0.490470	0.001809	0.713361
-9.648729	-2.024001	0.495475	0.001905	0.713357
-9.385754	-2.067956	0.500480	0.001856	0.713363
-9.569454	-2.039664	0.505485	0.001890	0.713354
-9.434449	-2.062584	0.510490	0.001865	0.713357
-9.847483	-2.137257	0.515494	0.001942	0.713062
-10.941141	-1.963736	0.520499	0.002145	0.713019
-10.468081	-2.044145	0.525504	0.002057	0.713027
-10.167913	-2.103514	0.530509	0.002001	0.713015
-10.765558	-1.993621	0.535514	0.002113	0.713022
-10.660492	-2.012581	0.540518	0.002093	0.713022
-10.396894	-2.089280	0.545523	0.002044	0.712962
-11.220328	-2.069453	0.550528	0.002197	0.712710
-11.100386	-2.094710	0.555533	0.002175	0.712702
-11.220375	-2.071296	0.560538	0.002197	0.712706
-11.187039	-2.074770	0.565542	0.002191	0.712711
-11.613952	-2.004274	0.570547	0.002270	0.712700
-11.262810	-2.062963	0.575552	0.002205	0.712708
-11.328465	-2.152399	0.580557	0.002217	0.712506
-12.740992	-1.962086	0.585562	0.002480	0.712384
-12.222408	-2.051514	0.590566	0.002384	0.712390
-11.900622	-2.112734	0.595571	0.002324	0.712382
-12.355183	-2.031509	0.600576	0.002408	0.712383
-12.429010	-2.020200	0.605581	0.002422	0.712379
-12.242686	-2.053325	0.610586	0.002388	0.712379
-12.228556	-2.155244	0.615590	0.002385	0.712181
-13.585255	-1.961918	0.620595	0.002637	0.712085
-12.899017	-2.082477	0.625600	0.002510	0.712088
-12.756922	-2.112070	0.630605	0.002483	0.712080
-13.352389	-2.005069	0.635610	0.002594	0.712081
-13.234882	-2.023936	0.640614	0.002572	0.712086
-13.141298	-2.043004	0.645619	0.002555	0.712081
-13.499859	-2.111164	0.650624	0.002622	0.711818
-14.409042	-1.980481	0.655629	0.002791	0.711755
-14.173723	-2.023160	0.660634	0.002747	0.711754
-13.765921	-2.094108	0.665638	0.002671	0.711757
-14.508478	-1.966533	0.670643	0.002809	0.711748
-14.167318	-2.022239	0.675648	0.002746	0.711758
-13.788635	-2.092266	0.680653	0.002675	0.711753
-14.307389	-2.090214	0.685658	0.002772	0.711573
-15.150718	-1.999388	0.690662	0.002929	0.711454
-14.808143	-2.065445	0.695667	0.002865	0.711444
-14.885756	-2.047785	0.700672	0.002880	0.711452
-15.456088	-1.949172	0.705677	0.002986	0.711446
-14.969245	-2.035224	0.710682	0.002895	0.711447
-14.591932	-2.100390	0.715686	0.002825	0.711451
-15.251843	-2.045678	0.720691	0.002948	0.711326
-15.918851	-2.021020	0.725696	0.003072	0.711138
-15.403799	-2.114409	0.730701	0.002976	0.711135
-15.901995	-2.024932	0.735706	0.003069	0.711136
-15.811342	-2.041012	0.740710	0.003052	0.711136
-15.715740	-2.062120	0.745715	0.003034	0.711128
-15.640357	-2.070746	0.750720	0.003020	0.711138
-15.973922	-2.088275	0.755725	0.003082	0.710984
-16.807941	-1.997017	0.760730	0.003237	0.710870
-16.545473	-2.041916	0.765734	0.003189	0.710873
-16.889588	-1.984118	0.770739	0.003253	0.710866
-16.717640	-2.011010	0.775744	0.003221	0.710874
-16.542066	-2.044413	0.780749	0.003188	0.710870
-16.851545	-1.989971	0.785754	0.003246	0.710868
-16.531416	-2.136388	0.790758	0.003186	0.710690
-17.857020	-1.979891	0.795763	0.003433	0.710531
-17.493284	-2.042253	0.800768	0.003365	0.710535
-17.795256	-1.991609	0.805773	0.003421	0.710529
-17.803570	-1.988413	0.810778	0.003423	0.710533
-17.336869	-2.069944	0.815782	0.003336	0.710536
-17.675993	-2.013852	0.820787	0.003399	0.710527
-17.754809	-2.051819	0.825792	0.003414	0.710423
-18.538799	-2.016063	0.830797	0.003560	0.710216
-18.137721	-2.086645	0.835802	0.003485	0.710217
-18.611961	-2.000416	0.840806	0.003573	0.710221
-18.694672	-1.990133	0.845811	0.003589	0.710212
-18.361240	-2.044402	0.850816	0.003527	0.710222
-18.406074	-2.040127	0.855821	0.003535	0.710215
-18.831291	-2.007745	0.860826	0.003614	0.710128
-19.357448	-2.029681	0.865830	0.003712	0.709897
-19.252498	-2.054674	0.870835	0.003693	0.709884
-19.414623	-2.020202	0.875840	0.003723	0.709895
-19.168713	-2.068716	0.880845	0.003677	0.709886
-19.578085	-1.994905	0.885850	0.003753	0.709888
-19.605910	-1.986945	0.890854	0.003758	0.709894
-19.413059	-2.036114	0.895859	0.003722	0.709864
-20.011651	-2.064293	0.900864	0.003834	0.709595
-20.421293	-1.993712	0.905869	0.003910	0.709590
-20.523175	-1.975364	0.910874	0.003929	0.709590
-19.623170	-2.132525	0.915878	0.003762	0.709597
-20.008955	-2.067678	0.920883	0.003833	0.709589
-20.220685	-2.025305	0.925888	0.003873	0.709598
-20.168660	-2.080938	0.930893	0.003863	0.709505
-21.102665	-2.037448	0.935898	0.004037	0.709259
-21.020714	-2.048587	0.940902	0.004022	0.709266
-21.665109	-1.938855	0.945907	0.004142	0.709256
-21.002839	-2.052834	0.950912	0.004018	0.709264
-21.026339	-2.050093	0.955917	0.004023	0.709261
-21.252507	-2.010608	0.960922	0.004065	0.709260
-21.028410	-2.065880	0.965926	0.004023	0.709229
-21.902721	-2.049935	0.970931	0.004186	0.708949
-22.041887	-2.019912	0.975936	0.004212	0.708959
-22.287323	-1.979721	0.980941	0.004257	0.708952
-22.249498	-1.985648	0.985946	0.004250	0.708954
-22.094342	-2.010926	0.990950	0.004222	0.708959
-22.320448	-1.974960	0.995955	0.004264	0.708950
-22.013352	-2.025525	1.000960	0.004206	0.708958
-22.340303	-2.076326	1.005965	0.004267	0.708740
-23.546919	-1.915564	1.010970	0.004492	0.708631
-22.744853	-2.055207	1.015974	0.004343	0.708638
-22.913470	-2.028939	1.020979	0.004374	0.708630
-23.135903	-1.986883	1.025984	0.004415	0.708635
-22.844760	-2.040570	1.030989	0.004361	0.708632
-22.745198	-2.057033	1.035994	0.004343	0.708634
-23.014905	-2.089389	1.040998	0.004393	0.708473
-24.089716	-1.962960	1.046003	0.004593	0.708343
-23.768401	-2.015988	1.051008	0.004533	0.708351
-23.805711	-2.010238	1.056013	0.004540	0.708349
-23.858246	-2.001813	1.061018	0.004550	0.708348
-23.630252	-2.038169	1.066022	0.004508	0.708356
-24.002171	-1.977182	1.071027	0.004577	0.708345
-23.897527	-2.088958	1.076032	0.004557	0.708159
-24.556335	-2.045675	1.081037	0.004680	0.708010
-24.473839	-2.061668	1.086042	0.004665	0.708008
-24.774832	-2.004559	1.091046	0.004721	0.708015
-24.952765	-1.978416	1.096051	0.004754	0.708003
-24.384929	-2.075931	1.101056	0.004648	0.708011
-24.671953	-2.026918	1.106061	0.004701	0.708007
-25.437210	-2.009869	1.111066	0.004844	0.707767
-25.552657	-2.022919	1.116070	0.004865	0.707700
-25.853777	-1.973493	1.121075	0.004921	0.707691
-25.676238	-2.000628	1.126080	0.004888	0.707700
-25.870089	-1.968999	1.131085	0.004924	0.707695
-25.753012	-1.991271	1.136090	0.004903	0.707692
-25.779095	-1.983319	1.141094	0.004908	0.707698
-25.752207	-2.010101	1.146099	0.004903	0.707654
-26.221104	-2.064559	1.151104	0.004990	0.707377
-26.196697	-2.069381	1.156109	0.004985	0.707376
-26.746164	-1.976968	1.161114	0.005088	0.707365
-26.588938	-1.999513	1.166118	0.005058	0.707376
-26.522295	-2.014857	1.171123	0.005046	0.707369
-26.767455	-1.969374	1.176128	0.005092	0.707373
-26.521488	-2.021038	1.181133	0.005046	0.707357
-27.072557	-2.064014	1.186138	0.005148	0.707074
-27.294627	-2.020196	1.191142	0.005190	0.707082
-27.734366	-1.947261	1.196147	0.005272	0.707071
-27.171711	-2.042775	1.201152	0.005167	0.707081
-27.312942	-2.018772	1.206157	0.005193	0.707079
-27.867064	-1.922181	1.211162	0.005296	0.707074
-27.447081	-1.993509	1.216166	0.005218	0.707081
-27.783529	-2.092324	1.221171	0.005281	0.706763
-28.429187	-1.982873	1.226176	0.005401	0.706751
-28.407145	-1.987467	1.231181	0.005397	0.706750
-28.225717	-2.021599	1.236186	0.005363	0.706746
-27.964356	-2.065510	1.241190	0.005314	0.706752
-28.401038	-1.992026	1.246195	0.005396	0.706743
-28.387265	-1.989978	1.251200	0.005393	0.706752
-28.755873	-2.075174	1.256205	0.005462	0.706449
-29.371656	-1.970111	1.261210	0.005576	0.706439
-29.192925	-1.999023	1.266214	0.005543	0.706445
-28.998822	-2.038249	1.271219	0.005507	0.706436
-29.229556	-1.992968	1.276224	0.005550	0.706444
-29.281371	-1.985056	1.281229	0.005560	0.706442
-29.200235	-2.001892	1.286234	0.005544	0.706437
-29.560334	-2.073120	1.291238	0.005612	0.706165
-30.447250	-1.936415	1.296243	0.005777	0.706122
-30.134488	-1.989765	1.301248	0.005718	0.706127
-29.833021	-2.044945	1.306253	0.005662	0.706124
-30.319972	-1.959931	1.311258	0.005753	0.706120
-30.188307	-1.981426	1.316262	0.005728	0.706124
-29.937370	-2.029074	1.321267	0.005682	0.706118
-30.257550	-2.067184	1.326272	0.005741	0.705927
-31.136198	-1.944323	1.331277	0.005905	0.705859
-30.974757	-1.974387	1.336282	0.005875	0.705857
-30.758184	-2.010398	1.341286	0.005834	0.705862
-31.112356	-1.951457	1.346291	0.005900	0.705853
-30.992539	-1.968086	1.351296	0.005878	0.705863
-30.868609	-1.990415	1.356301	0.005855	0.705862
-31.144576	-2.066009	1.361306	0.005906	0.705611
-32.007961	-1.954965	1.366310	0.006067	0.705525
-31.836489	-1.989881	1.371315	0.006035	0.705516
-31.641567	-2.021725	1.376320	0.005999	0.705522
-31.816600	-1.992388	1.381325	0.006032	0.705519
-31.835812	-1.989976	1.386330	0.006035	0.705516
-31.677816	-2.014267	1.391334	0.006006	0.705524
-32.511480	-1.998325	1.396339	0.006161	0.705257
-32.794787	-1.972715	1.401344	0.006214	0.705207
-32.469267	-2.031604	1.406349	0.006153	0.705205
-32.746753	-1.984040	1.411354	0.006205	0.705202
-32.787404	-1.972571	1.416358	0.006212	0.705210
-32.599348	-2.010442	1.421363	0.006177	0.705201
-32.403551	-2.042560	1.426368	0.006141	0.705207
-33.224273	-2.036030	1.431373	0.006294	0.704926
-33.824555	-1.953743	1.436378	0.006405	0.704876
-33.572036	-1.992991	1.441382	0.006358	0.704887
-33.733609	-1.968570	1.446387	0.006388	0.704879
-33.815116	-1.950439	1.451392	0.006404	0.704886
-33.609759	-1.987558	1.456397	0.006365	0.704885
-33.801637	-1.957191	1.461402	0.006401	0.704877
-33.902737	-1.992683	1.466406	0.006420	0.704769
-34.834195	-1.922664	1.471411	0.006593	0.704576
-34.194164	-2.033132	1.476416	0.006474	0.704583
-34.610231	-1.957837	1.481421	0.006552	0.704585
-34.928651	-1.903010	1.486426	0.006611	0.704582
-34.350313	-2.002169	1.491430	0.006503	0.704589
-34.778899	-1.930916	1.496435	0.006583	0.704579
-34.739572	-1.936809	1.501440	0.006576	0.704581
-34.572724	-2.128896	1.506445	0.006545	0.704254
-35.216512	-2.015556	1.511450	0.006664	0.704251
-35.509883	-1.958030	1.516454	0.006719	0.704262
-35.145038	-2.028501	1.521459	0.006651	0.704251
-35.014326	-2.050492	1.526464	0.006627	0.704254
-35.617041	-1.941455	1.531469	0.006739	0.704257
-35.455035	-2.050436	1.536474	0.006709	0.704095
-36.083146	-2.008625	1.541478	0.006826	0.703954
-36.191132	-1.993827	1.546483	0.006846	0.703945
-36.314519	-1.970710	1.551488	0.006869	0.703947
-36.271616	-1.977319	1.556493	0.006861	0.703949
-36.272292	-1.979872	1.561498	0.006861	0.703944
-36.335024	-1.965712	1.566502	0.006873	0.703950
-36.500746	-1.998391	1.571507	0.006904	0.703824
-37.009948	-2.002738	1.576512	0.006998	0.703632
-36.848755	-2.031056	1.581517	0.006968	0.703633
-37.089535	-1.991651	1.586522	0.007013	0.703626
-36.783993	-2.042495	1.591526	0.006956	0.703633
-37.145280	-1.983887	1.596531	0.007024	0.703622
-37.191955	-1.972088	1.601536	0.007032	0.703629
-37.021769	-2.101789	1.606541	0.007001	0.703428
-38.043204	-1.967662	1.611546	0.007191	0.703331
-37.848452	-1.996822	1.616550	0.007154	0.703343
-37.985126	-1.976092	1.621555	0.007180	0.703335
-37.661560	-2.032240	1.626560	0.007120	0.703338
-37.772777	-2.013999	1.631565	0.007140	0.703335
-38.076829	-1.965399	1.636570	0.007197	0.703324
-38.500739	-2.046483	1.641574	0.007276	0.703008
-38.651540	-2.024005	1.646579	0.007304	0.702999
-38.984973	-1.964056	1.651584	0.007366	0.703000
-38.735959	-2.007918	1.656589	0.007320	0.703001
-38.689403	-2.018774	1.661594	0.007311	0.702996
-38.723630	-2.006994	1.666598	0.007317	0.703007
-39.095074	-1.950663	1.671603	0.007386	0.702987
-39.341402	-2.055953	1.676608	0.007432	0.702686
-39.612267	-2.005536	1.681613	0.007483	0.702690
-40.000202	-1.940890	1.686618	0.007555	0.702681
-39.316299	-2.058510	1.691622	0.007428	0.702690
-39.615835	-2.009007	1.696627	0.007483	0.702682
-40.007265	-1.936707	1.701632	0.007556	0.702687
-39.799769	-1.972897	1.706637	0.007518	0.702688
-40.333405	-2.033223	1.711642	0.007617	0.702374
-40.733491	-1.963665	1.716646	0.007692	0.702371
-40.817997	-1.952385	1.721651	0.007707	0.702363
-40.169657	-2.067606	1.726656	0.007587	0.702364
-40.353143	-2.033388	1.731661	0.007621	0.702367
-40.925145	-1.934797	1.736666	0.007727	0.702360
-40.137812	-2.073760	1.741670	0.007581	0.702363
-40.780907	-2.106350	1.746675	0.007700	0.702065
-41.604685	-1.958115	1.751680	0.007854	0.702068
-41.518939	-1.971132	1.756685	0.007838	0.702072
-41.209739	-2.029434	1.761690	0.007780	0.702066
-41.139175	-2.039396	1.766694	0.007767	0.702071
-41.583747	-1.963718	1.771699	0.007850	0.702064
-41.182410	-2.088650	1.776704	0.007775	0.701956
-42.052774	-2.039315	1.781709	0.007937	0.701742
-42.404948	-1.979761	1.786714	0.008003	0.701735
-42.029603	-2.041951	1.791718	0.007933	0.701745
-42.168166	-2.020564	1.796723	0.007959	0.701738
-42.450389	-1.967582	1.801728	0.008011	0.701744
-42.607051	-1.940963	1.806733	0.008040	0.701741
-42.611166	-1.971320	1.811738	0.008041	0.701678
-43.091437	-2.005145	1.816742	0.008131	0.701436
-43.246972	-1.980151	1.821747	0.008159	0.701431
-43.180967	-1.989150	1.826752	0.008147	0.701436
-42.856901	-2.047172	1.831757	0.008087	0.701436
-43.636868	-1.911525	1.836762	0.008232	0.701429
-43.334867	-1.961141	1.841766	0.008176	0.701437
-42.959525	-2.043805	1.846771	0.008106	0.701406
-43.825699	-2.030423	1.851776	0.008267	0.701120
-44.118881	-1.976413	1.856781	0.008322	0.701124
-44.135954	-1.977842	1.861786	0.008325	0.701114
-43.638644	-2.063291	1.866790	0.008232	0.701121
-44.216624	-1.963427	1.871795	0.008340	0.701115
-44.360134	-1.937686	1.876800	0.008367	0.701115
-43.811005	-2.048598	1.881805	0.008264	0.701089
-44.799368	-1.982850	1.886810	0.008448	0.700865
-45.044576	-1.935930	1.891814	0.008494	0.700871
-44.872476	-1.969590	1.896819	0.008462	0.700865
-44.966494	-1.952174	1.901824	0.008480	0.700866
-44.931390	-1.956396	1.906829	0.008473	0.700871
-44.896150	-1.965843	1.911834	0.008466	0.700864
-44.787312	-2.012759	1.916838	0.008446	0.700808
-46.103010	-1.917118	1.921843	0.008691	0.700527
-45.660969	-1.993910	1.926848	0.008609	0.700531
-45.389467	-2.040252	1.931853	0.008558	0.700535
-45.878854	-1.958336	1.936858	0.008649	0.700524
-45.724933	-1.983440	1.941862	0.008621	0.700529
-45.880120	-1.957964	1.946867	0.008650	0.700525
-45.624417	-2.045262	1.951872	0.008602	0.700440
-46.806697	-1.944779	1.956877	0.008822	0.700216
-46.706319	-1.966070	1.961882	0.008803	0.700209
-46.457996	-2.006895	1.966886	0.008757	0.700216
-46.746460	-1.959113	1.971891	0.008811	0.700209
-46.768378	-1.953823	1.976896	0.008815	0.700212
-46.282499	-2.038513	1.981901	0.008725	0.700216
-46.561740	-2.049017	1.986906	0.008777	0.700094
-47.496041	-1.979695	1.991910	0.008950	0.699896
-47.264155	-2.025246	1.996915	0.008907	0.699888
-47.624748	-1.958336	2.001920	0.008974	0.699893
-47.363275	-2.005437	2.011917	0.008926	0.699892
-47.613871	-1.961448	2.021914	0.008972	0.699891
-47.760055	-2.014061	2.031910	0.009000	0.699731
-48.481558	-1.925478	2.041907	0.009134	0.699650
-47.920898	-2.051153	2.051904	0.009030	0.699597
-47.913717	-1.957417	2.061901	0.009028	0.699790
-47.735561	-1.995782	2.071898	0.008995	0.699777
-47.791118	-1.929002	2.081894	0.009005	0.699892
-47.298332	-2.017316	2.091891	0.008914	0.699892
-47.456195	-1.989480	2.101888	0.008943	0.699891
-47.537223	-1.975192	2.111885	0.008958	0.699891
-47.726201	-1.942384	2.121882	0.008993	0.699889
-47.326153	-2.013620	2.131878	0.008919	0.699889
-47.508501	-1.980647	2.141875	0.008953	0.699890
-46.934128	-1.994030	2.151872	0.008846	0.700071
-46.799613	-1.948406	2.161869	0.008821	0.700212
-46.495424	-2.002199	2.171866	0.008764	0.700213
-46.443549	-2.010302	2.181862	0.008754	0.700215
-46.627497	-1.975541	2.191859	0.008789	0.700219
-46.007377	-1.949124	2.201856	0.008673	0.700497
-45.783337	-1.971815	2.211853	0.008631	0.700532
-45.733142	-1.981391	2.221850	0.008622	0.700531
-45.835282	-1.964688	2.231846	0.008641	0.700528
-45.124514	-1.935511	2.241843	0.008509	0.700844
-44.606269	-2.012854	2.251840	0.008412	0.700874
-44.749210	-1.989455	2.261837	0.008439	0.700870
-44.814381	-1.978845	2.271834	0.008451	0.700868
-44.381146	-1.942192	2.281830	0.008370	0.701099
-44.140485	-1.975161	2.291827	0.008325	0.701119
-43.966984	-2.006069	2.301824	0.008293	0.701119
-43.922645	-1.942672	2.311821	0.008285	0.701263
-43.228290	-1.984129	2.321818	0.008156	0.701430
-43.216242	-1.987521	2.331814	0.008153	0.701428
-43.231657	-1.984511	2.341811	0.008156	0.701428
-42.458324	-1.974575	2.351808	0.008012	0.701728
-42.554189	-1.952198	2.361805	0.008030	0.701738
-42.102698	-2.033254	2.371802	0.007946	0.701737
-42.127444	-1.968906	2.381798	0.007951	0.701858
-41.380851	-1.997227	2.391795	0.007811	0.702070
-41.413112	-1.992140	2.401792	0.007817	0.702069
-41.432735	-1.990852	2.411789	0.007821	0.702065
-40.755449	-1.988653	2.421786	0.007695	0.702313
-40.675380	-1.978315	2.431782	0.007680	0.702363
-40.618165	-1.987791	2.441779	0.007669	0.702365
-40.324657	-1.974604	2.451776	0.007615	0.702497
-39.830380	-1.968931	2.461773	0.007523	0.702687
-39.671833	-1.997750	2.471770	0.007493	0.702686
-39.846421	-1.965353	2.481766	0.007526	0.702688
-39.076562	-1.954043	2.491763	0.007382	0.702988
-38.687128	-2.014820	2.501760	0.007310	0.703006
-38.758312	-2.002717	2.511757	0.007323	0.703005
-38.692506	-1.958658	2.521754	0.007311	0.703117
-37.967416	-1.978176	2.531750	0.007176	0.703339
-37.948318	-1.980428	2.541747	0.007172	0.703341
-38.051271	-1.963861	2.551744	0.007191	0.703338
-37.350613	-1.950133	2.561741	0.007061	0.703618
-36.921938	-2.020529	2.571738	0.006981	0.703630
-37.010885	-2.002587	2.581734	0.006998	0.703634
-36.907695	-1.965334	2.591731	0.006978	0.703746
-36.235703	-1.985119	2.601728	0.006853	0.703948
-36.282540	-1.976002	2.611725	0.006862	0.703950
-36.181628	-1.994157	2.621722	0.006843	0.703949
-35.508481	-1.967484	2.631718	0.006718	0.704245
-35.334569	-1.992296	2.641715	0.006685	0.704258
-35.458948	-1.969703	2.651712	0.006709	0.704258
-35.180469	-1.929139	2.661709	0.006657	0.704440
-34.538066	-1.973406	2.671706	0.006537	0.704582
-34.784837	-1.929149	2.681702	0.006583	0.704582
-34.327913	-1.978269	2.691699	0.006498	0.704648
-33.809609	-1.951734	2.701696	0.006401	0.704887
-33.492942	-2.010369	2.711693	0.006343	0.704883
-33.619739	-1.987695	2.721690	0.006366	0.704883
-33.148464	-1.965076	2.731686	0.006278	0.705098
-32.763799	-1.977723	2.741683	0.006207	0.705210
-32.644477	-1.999197	2.751680	0.006184	0.705210
-32.505606	-2.021556	2.761677	0.006159	0.705215
-31.922720	-1.973262	2.771674	0.006050	0.705521
-31.552973	-2.039573	2.781670	0.005981	0.705520
-31.606912	-2.028529	2.791667	0.005991	0.705523
-31.771036	-1.944861	2.801664	0.006022	0.705633
-30.877145	-1.992172	2.811661	0.005855	0.705858
-30.838434	-1.997721	2.821658	0.005848	0.705861
-30.979244	-1.972317	2.831654	0.005874	0.705862
-30.069306	-2.026606	2.841651	0.005705	0.706079
-30.263521	-1.967582	2.851648	0.005741	0.706128
-29.920542	-2.029702	2.861645	0.005677	0.706126
-30.252780	-1.914192	2.871642	0.005739	0.706239
-29.357499	-1.972572	2.881638	0.005572	0.706442
-29.309913	-1.980441	2.891635	0.005563	0.706444
-29.449936	-1.930792	2.901632	0.005589	0.706493
-28.594073	-1.954830	2.911629	0.005430	0.706751
-28.399493	-1.990106	2.921626	0.005394	0.706750
-28.426360	-1.985831	2.931622	0.005399	0.706749
-27.711971	-1.984288	2.941619	0.005266	0.707008
-27.636161	-1.959973	2.951616	0.005252	0.707084
-27.464789	-1.992474	2.961613	0.005220	0.707080
-27.770099	-1.889359	2.971610	0.005277	0.707178
-26.564895	-2.004855	2.981606	0.005052	0.707377
-26.685542	-1.982619	2.991603	0.005075	0.707379
-26.623810	-1.994487	3.001600	0.005063	0.707377
-26.174657	-1.935685	3.011597	0.004980	0.707656
-26.029709	-1.941502	3.021594	0.004953	0.707696
-25.592951	-2.018735	3.031590	0.004871	0.707697
-25.551416	-1.951289	3.041587	0.004863	0.707847
-25.011940	-1.964041	3.051584	0.004763	0.708014
-24.893669	-1.984973	3.061581	0.004741	0.708015
-25.050839	-1.957709	3.071578	0.004770	0.708013
-24.095332	-1.961839	3.081574	0.004592	0.708346
-23.894476	-1.995111	3.091571	0.004555	0.708351
-24.094524	-1.959425	3.101568	0.004592	0.708351
-23.804261	-1.951334	3.111565	0.004538	0.708471
-23.262292	-1.966205	3.121562	0.004437	0.708635
-23.263531	-1.964666	3.131558	0.004437	0.708638
-23.463619	-1.908215	3.141555	0.004475	0.708679
-22.272267	-1.981809	3.151552	0.004253	0.708957
-22.171115	-1.999337	3.161549	0.004234	0.708958
-22.484533	-1.945360	3.171546	0.004292	0.708954
-22.023464	-1.944892	3.181542	0.004206	0.709120
-21.420345	-1.979405	3.191539	0.004094	0.709266
-21.420453	-1.980331	3.201536	0.004094	0.709264
-21.464876	-1.962971	3.211533	0.004102	0.709283
-20.792567	-1.928025	3.221530	0.003977	0.709593
-20.303067	-2.014529	3.231526	0.003886	0.709594
-20.640043	-1.952333	3.241523	0.003949	0.709598
-20.255370	-1.944694	3.251520	0.003877	0.709751
-19.683458	-1.976231	3.261517	0.003771	0.709892
-19.674415	-1.979024	3.271514	0.003769	0.709889
-19.671561	-1.974654	3.281510	0.003768	0.709899
-18.734475	-1.982798	3.291507	0.003594	0.710216
-18.725822	-1.983840	3.301504	0.003592	0.710217
-18.751708	-1.979744	3.311501	0.003597	0.710216
-18.665298	-1.946613	3.321498	0.003581	0.710313
-17.646516	-2.020357	3.331494	0.003391	0.710529
-17.573834	-2.031753	3.341491	0.003378	0.710532
-17.508704	-2.041881	3.351488	0.003366	0.710535
-17.273683	-1.991260	3.361485	0.003322	0.710720
-16.664214	-2.024566	3.371482	0.003208	0.710870
-16.906545	-1.980255	3.381478	0.003254	0.710872
-16.927589	-1.976787	3.391475	0.003257	0.710872
-15.959718	-2.036938	3.401472	0.003077	0.711096
-15.983567	-2.011510	3.411469	0.003082	0.711138
-15.823423	-2.040252	3.421466	0.003052	0.711138
-15.840527	-2.024210	3.431462	0.003055	0.711164
-14.971889	-2.033714	3.441459	0.002893	0.711454
-15.007586	-2.027636	3.451456	0.002900	0.711453
-15.119554	-2.008045	3.461453	0.002921	0.711452
-14.588399	-2.029739	3.471450	0.002822	0.711598
-14.002917	-2.052277	3.481446	0.002713	0.711761
-14.020421	-2.047951	3.491443	0.002716	0.711763
-14.229539	-2.010931	3.501440	0.002755	0.711763
-13.364167	-2.024857	3.511437	0.002594	0.712043
-13.186249	-2.034803	3.521434	0.002561	0.712086
-13.142080	-2.041309	3.531430	0.002552	0.712089
-13.088571	-2.015985	3.541427	0.002542	0.712158
-12.375305	-2.028736	3.551424	0.002410	0.712386
-12.488575	-2.009738	3.561421	0.002431	0.712384
-12.172941	-2.066340	3.571418	0.002372	0.712383
-11.881026	-2.005112	3.581414	0.002318	0.712608
-11.500598	-2.022703	3.591411	0.002247	0.712708
-11.470922	-2.027214	3.601408	0.002241	0.712710
-11.513344	-1.976953	3.611405	0.002249	0.712795
-10.294647	-2.079686	3.621402	0.002022	0.713023
-10.333681	-2.071875	3.631398	0.002029	0.713024
-10.449927	-2.051211	3.641395	0.002051	0.713024
-10.198673	-2.009066	3.651392	0.002004	0.713197
-9.512754	-2.048627	3.661389	0.001877	0.713362
-9.532547	-2.046445	3.671386	0.001880	0.713359
-9.549068	-2.044217	3.681382	0.001883	0.713358
-8.806187	-2.054484	3.691379	0.001745	0.713601
-8.731632	-2.040693	3.701376	0.001731	0.713654
-8.402987	-2.099019	3.711373	0.001670	0.713655
-8.491153	-2.077384	3.721370	0.001686	0.713667
-7.942658	-2.023703	3.731366	0.001584	0.713968
-7.647185	-2.074544	3.741363	0.001529	0.713971
-7.662716	-2.070920	3.751360	0.001532	0.713973
-7.639752	-2.007529	3.761357	0.001528	0.714107
-6.779636	-2.075448	3.771354	0.001368	0.714277
-6.985170	-2.039193	3.781350	0.001406	0.714276
-6.838819	-2.063072	3.791347	0.001379	0.714280
-6.252703	-2.000247	3.801344	0.001269	0.714612
-5.951776	-2.056228	3.811341	0.001213	0.714608
-5.952951	-2.056421	3.821338	0.001214	0.714607
-5.809059	-2.013014	3.831334	0.001187	0.714744
-4.858126	-2.099665	3.841331	0.001010	0.714908
-5.139358	-2.048311	3.851328	0.001062	0.714911
-4.977950	-2.076838	3.861325	0.001032	0.714911
-4.413754	-2.042176	3.871322	0.000927	0.715179
-4.253664	-2.043756	3.881318	0.000897	0.715233
-4.023754	-2.083934	3.891315	0.000854	0.715234
-4.174796	-2.017830	3.901312	0.000882	0.715312
-3.363187	-2.043677	3.911309	0.000731	0.715548
-3.135988	-2.086327	3.921306	0.000689	0.715543
-3.186661	-2.076796	3.931302	0.000698	0.715544
-2.740844	-2.049424	3.941299	0.000615	0.715756
-2.462094	-2.033669	3.951296	0.000564	0.715886
-2.293539	-2.065873	3.961293	0.000532	0.715881
-2.488750	-2.021444	3.971290	0.000568	0.715901
-1.755502	-2.036657	3.981286	0.000432	0.716129
-1.751403	-2.035856	3.991283	0.000431	0.716132
-1.580644	-2.066362	4.001280	0.000399	0.716132
-1.931481	-1.880805	4.011277	0.000465	0.716376
-1.466863	-1.926596	4.021274	0.000378	0.716449
-1.520951	-1.891985	4.031270	0.000388	0.716499
-1.160146	-1.827088	4.041267	0.000321	0.716754
-0.844024	-1.882459	4.051264	0.000262	0.716756
-0.781594	-1.788420	4.061261	0.000250	0.716964
-0.933806	-1.701392	4.071258	0.000279	0.717083
-1.031741	-1.621534	4.081254	0.000297	0.717206
-0.972626	-1.544188	4.091251	0.000286	0.717380
-0.764252	-1.497478	4.101248	0.000247	0.717546
-0.815308	-1.407980	4.111245	0.000256	0.717705
-0.617983	-1.327228	4.121242	0.000220	0.717934
-0.693472	-1.259284	4.131238	0.000234	0.718042
-0.753149	-1.090914	4.141235	0.000245	0.718353
-0.588495	-1.038161	4.151232	0.000214	0.718515
-0.482018	-0.974473	4.161229	0.000194	0.718678
-0.512967	-0.827873	4.171226	0.000200	0.718957
-0.504178	-0.711752	4.181222	0.000198	0.719189
-0.334814	-0.629264	4.191219	0.000166	0.719411
-0.296947	-0.513172	4.201216	0.000159	0.719653
-0.499041	-0.351607	4.211213	0.000197	0.719901
-0.292272	-0.225557	4.221210	0.000158	0.720222
-0.215747	-0.103549	4.231206	0.000144	0.720489
-0.099100	0.024111	4.241203	0.000122	0.720781
0.000000	0.143937	4.251200	0.000103	0.721052
-0.114668	0.788067	4.256205	0.000124	0.722278
0.005237	2.034469	4.261210	0.000101	0.724763
0.416542	3.822284	4.266214	0.000023	0.728397
0.712102	6.182850	4.271219	-0.000033	0.733081
0.809922	9.085550	4.276224	-0.000053	0.738710
1.198062	12.413818	4.281229	-0.000128	0.745205
1.472447	16.220173	4.286234	-0.000181	0.752507
1.742700	20.432019	4.291238	-0.000234	0.760495
2.006001	25.033293	4.296243	-0.000286	0.769116
2.631509	29.950075	4.301248	-0.000406	0.778333
2.983031	35.257020	4.306253	-0.000475	0.788057
3.400646	40.870897	4.311258	-0.000556	0.798229
3.988509	46.761983	4.316262	-0.000670	0.808812
4.325614	52.974387	4.321267	-0.000737	0.819737
4.761095	59.449125	4.326272	-0.000822	0.830996
5.245008	66.135416	4.331277	-0.000916	0.842475
5.717511	73.040530	4.336282	-0.001009	0.854159
6.290822	80.139300	4.341286	-0.001120	0.866032
6.664690	87.457309	4.346291	-0.001195	0.878041
11.047612	94.268910	4.351296	-0.002015	0.890204
12.849446	101.763111	4.356301	-0.002355	0.902561
13.198232	109.651339	4.361306	-0.002426	0.914966
13.775306	117.607974	4.366310	-0.002538	0.927370
14.499607	125.652812	4.371315	-0.002678	0.939782
15.495734	133.760967	4.376320	-0.002869	0.952197
16.537870	141.954695	4.381325	-0.003068	0.964589
17.129976	150.300307	4.386330	-0.003184	0.976930
18.318880	158.641463	4.391334	-0.003411	0.989259
19.135809	167.091532	4.396339	-0.003569	1.001499
19.866884	175.586132	4.401344	-0.003710	1.013631
21.007784	184.048464	4.406349	-0.003928	1.025673
21.918313	192.586439	4.411354	-0.004103	1.037624
23.046826	201.120200	4.416358	-0.004319	1.049483
23.774557	209.745074	4.421363	-0.004460	1.061238
24.821099	218.351775	4.426368	-0.004661	1.072913
25.678025	226.994101	4.431373	-0.004826	1.084465
26.371924	235.668400	4.436378	-0.004961	1.095900
26.908862	244.371907	4.441382	-0.005066	1.107220
27.736717	253.023360	4.446387	-0.005226	1.118421
28.561893	261.657557	4.451392	-0.005385	1.129490
29.530738	270.288345	4.456397	-0.005571	1.140476
30.556807	278.925809	4.461402	-0.005768	1.151378
31.597551	287.541765	4.466406	-0.005968	1.162153
32.661832	296.128992	4.471411	-0.006171	1.172800
33.353409	304.778186	4.476416	-0.006306	1.183348
33.890251	313.446359	4.481421	-0.006411	1.193793
34.349761	322.075540	4.486426	-0.006503	1.204086
35.389111	330.630107	4.491430	-0.006702	1.214320
36.362951	339.160693	4.496435	-0.006889	1.224427
36.986489	347.775786	4.501440	-0.007010	1.234480
37.610461	356.338746	4.506445	-0.007132	1.244392
38.569017	364.841494	4.511450	-0.007316	1.254221
39.254392	373.379264	4.516454	-0.007449	1.263961
39.976285	381.895969	4.521459	-0.007589	1.273609
40.810167	390.370472	4.526464	-0.007750	1.283159
41.503489	398.881301	4.531469	-0.007885	1.292652
41.749019	407.421272	4.536474	-0.007936	1.302025
42.423092	415.970120	4.541478	-0.008067	1.311418
43.194662	424.436926	4.546483	-0.008216	1.320673
43.899817	432.849135	4.551488	-0.008353	1.329794
44.625300	441.263930	4.556493	-0.008494	1.338859
45.649943	449.604189	4.561498	-0.008690	1.347836
46.403682	458.014752	4.566502	-0.008836	1.356780
46.816675	466.428289	4.571507	-0.008918	1.365609
47.073541	474.874859	4.576512	-0.008971	1.374389
47.812099	483.223492	4.581517	-0.009114	1.383094
48.330787	491.606769	4.586522	-0.009216	1.391743
49.323364	499.910327	4.591526	-0.009407	1.400337
49.911977	508.252149	4.596531	-0.009522	1.408849
50.610090	516.596335	4.601536	-0.009657	1.417331
51.092787	524.949889	4.606541	-0.009752	1.425735
51.646086	533.295877	4.611546	-0.009861	1.434094
52.591644	541.563045	4.616550	-0.010042	1.442391
52.962739	549.915891	4.621555	-0.010117	1.450631
53.580463	558.226289	4.626560	-0.010237	1.458823
54.776817	566.437254	4.631565	-0.010465	1.466964
55.224422	574.828052	4.636570	-0.010554	1.475114
55.825758	583.116214	4.641574	-0.010672	1.483146
56.426918	591.384634	4.646579	-0.010789	1.491115
57.123155	599.661300	4.651584	-0.010924	1.499065
57.565019	607.958781	4.656589	-0.011012	1.506952
58.321915	616.209463	4.661594	-0.011158	1.514803
58.951120	624.467372	4.666598	-0.011281	1.522600
59.188986	632.777279	4.671603	-0.011330	1.530347
59.662254	641.054651	4.676608	-0.011424	1.538059
60.351736	649.268459	4.681613	-0.011558	1.545707
60.716562	657.571987	4.686618	-0.011631	1.553351
61.364274	665.779120	4.691622	-0.011757	1.560911
61.921369	674.007122	4.696627	-0.011866	1.568440
62.422178	682.249728	4.701632	-0.011965	1.575938
62.899751	690.485201	4.706637	-0.012059	1.583391
63.660483	698.675411	4.711642	-0.012206	1.590808
64.403061	706.885864	4.716646	-0.012349	1.598207
64.573660	715.144298	4.721651	-0.012387	1.605532
65.108121	723.365281	4.726656	-0.012491	1.612842
65.812991	731.561393	4.731661	-0.012628	1.620122
66.081233	739.800486	4.736666	-0.012683	1.627345
66.453568	748.097567	4.741670	-0.012758	1.634600
66.875938	756.275960	4.746675	-0.012842	1.641728
67.283112	764.465570	4.751680	-0.012923	1.648833
67.900337	772.648254	4.756685	-0.013044	1.655930
68.379642	780.821040	4.761690	-0.013138	1.662969
69.125563	788.982270	4.766694	-0.013282	1.670004
69.259952	797.228593	4.771699	-0.013313	1.676999
69.480173	805.432087	4.776704	-0.013359	1.683941
70.322678	813.578737	4.781709	-0.013521	1.690889
70.672877	821.774336	4.786714	-0.013592	1.697784
71.123197	829.953852	4.791718	-0.013681	1.704651
71.757148	838.127360	4.796723	-0.013804	1.711510
72.603732	846.242728	4.801728	-0.013967	1.718320
72.871957	854.430757	4.806733	-0.014023	1.725088
73.346210	862.598675	4.811738	-0.014116	1.731840
73.812496	870.778578	4.816742	-0.014208	1.738574
74.274175	878.925426	4.821747	-0.014300	1.745254
74.873047	887.086013	4.826752	-0.014416	1.751938
75.315066	895.271678	4.831757	-0.014504	1.758596
75.558961	903.423406	4.836762	-0.014555	1.765177
75.860762	911.632952	4.841766	-0.014616	1.771786
76.013104	919.826936	4.846771	-0.014650	1.778341
76.427706	927.960200	4.851776	-0.014733	1.784855
76.733143	936.175123	4.856781	-0.014795	1.791396
76.990888	944.348103	4.861786	-0.014848	1.797875
77.361984	952.467644	4.866790	-0.014923	1.804302
77.950913	960.566674	4.871795	-0.015038	1.810717
78.404036	968.704762	4.876800	-0.015127	1.817123
78.884152	976.833079	4.881805	-0.015222	1.823502
78.973066	985.008821	4.886810	-0.015244	1.829848
79.165725	993.184552	4.891814	-0.015285	1.836185
79.601148	1001.278710	4.896819	-0.015371	1.842466
79.980156	1009.415078	4.901824	-0.015447	1.848751
80.353054	1017.570018	4.906829	-0.015522	1.855029
80.587453	1025.704771	4.911834	-0.015571	1.861253
80.954431	1033.836852	4.916838	-0.015645	1.867470
81.511462	1041.975653	4.921843	-0.015754	1.873693
81.708070	1050.106389	4.926848	-0.015796	1.879848
82.032581	1058.230988	4.931853	-0.015861	1.885993
82.585194	1066.325814	4.936858	-0.015969	1.892122
82.862496	1074.481878	4.941862	-0.016026	1.898245
83.263635	1082.584657	4.946867	-0.016106	1.904322
83.771016	1090.694452	4.951872	-0.016206	1.910398
84.176421	1098.837927	4.956877	-0.016287	1.916467
84.204055	1106.984089	4.961882	-0.016297	1.922477
84.692270	1115.092482	4.966886	-0.016394	1.928492
84.936583	1123.229672	4.971891	-0.016444	1.934481
85.265691	1131.337828	4.976896	-0.016511	1.940441
85.581210	1139.460380	4.981901	-0.016575	1.946391
86.084825	1147.583301	4.986906	-0.016674	1.952344
86.483057	1155.711839	4.991910	-0.016753	1.958270
86.591742	1163.818797	4.996915	-0.016779	1.964133
86.979862	1171.902240	5.001920	-0.016857	1.969990
87.202443	1180.052672	5.006925	-0.016903	1.975861
87.443346	1188.146354	5.011930	-0.016953	1.981676
87.975558	1196.233157	5.016934	-0.017058	1.987499
88.115106	1204.377241	5.021939	-0.017089	1.993305
88.291597	1212.488565	5.026944	-0.017127	1.999074
88.652629	1220.571799	5.031949	-0.017200	2.004826
88.965765	1228.671687	5.036954	-0.017263	2.010568
89.320147	1236.787351	5.041958	-0.017335	2.016310
89.510908	1244.899103	5.046963	-0.017375	2.022015
89.915251	1252.984544	5.051968	-0.017456	2.027707
90.198562	1261.147218	5.056973	-0.017514	2.033425
90.172944	1269.266552	5.061978	-0.017515	2.039066
90.784550	1277.293776	5.066982	-0.017634	2.044691
90.981202	1285.408340	5.071987	-0.017676	2.050320
91.365285	1293.485258	5.076992	-0.017752	2.055925
91.821243	1301.569480	5.081997	-0.017843	2.061528
92.088673	1309.655055	5.087002	-0.017898	2.067098
92.384848	1317.787966	5.092006	-0.017958	2.072687
92.568433	1325.906534	5.097011	-0.017998	2.078241
92.906911	1333.966512	5.102016	-0.018066	2.083755
93.279047	1342.062129	5.107021	-0.018140	2.089282
93.609980	1350.170682	5.112026	-0.018207	2.094799
93.714178	1358.298533	5.117030	-0.018232	2.100293
94.184350	1366.357852	5.122035	-0.018325	2.105761
94.121233	1374.524905	5.127040	-0.018318	2.111236
94.549713	1382.636090	5.132045	-0.018404	2.116706
94.709690	1390.695642	5.137050	-0.018439	2.122103
95.183516	1398.747796	5.142054	-0.018532	2.127510
95.253978	1406.873629	5.147059	-0.018550	2.132915
95.579178	1414.943463	5.152064	-0.018616	2.138292
95.929659	1423.011567	5.157069	-0.018687	2.143657
96.199009	1431.081908	5.162074	-0.018742	2.149003
96.549673	1439.189456	5.167078	-0.018813	2.154368
97.034048	1447.225727	5.172083	-0.018908	2.159684
97.066775	1455.326036	5.177088	-0.018920	2.164988
97.328706	1463.437076	5.182093	-0.018974	2.170306
97.748967	1471.491702	5.187098	-0.019057	2.175590
98.143847	1479.575131	5.192102	-0.019136	2.180877
98.146965	1487.684351	5.197107	-0.019142	2.186132
98.449836	1495.778871	5.202112	-0.019204	2.191392
98.822874	1503.869341	5.207117	-0.019278	2.196643
98.955196	1511.925994	5.212122	-0.019308	2.201838
99.391898	1519.986134	5.217126	-0.019395	2.207050
99.818869	1528.056779	5.222131	-0.019479	2.212256
100.075605	1536.151616	5.227136	-0.019533	2.217450
100.258349	1544.248311	5.232141	-0.019572	2.222626
100.636582	1552.299248	5.237146	-0.019648	2.227779
100.915016	1560.412650	5.242150	-0.019705	2.232950
101.332811	1568.466812	5.247155	-0.019788	2.238084
101.664785	1576.517359	5.252160	-0.019855	2.243196
102.477569	1584.538573	5.257165	-0.020011	2.248320
102.840562	1592.636094	5.262170	-0.020084	2.253441
103.015362	1600.749568	5.267174	-0.020122	2.258544
103.277509	1608.821441	5.272179	-0.020176	2.263617
103.391394	1616.926670	5.277184	-0.020203	2.268687
103.818665	1625.079993	5.282189	-0.020288	2.273802
104.076049	1633.118565	5.287194	-0.020341	2.278819
104.372974	1641.171855	5.292198	-0.020401	2.283839
104.489965	1649.256019	5.297203	-0.020428	2.288850
104.806051	1657.317674	5.302208	-0.020492	2.293854
105.392565	1665.348565	5.307213	-0.020607	2.298851
105.532336	1673.419532	5.312218	-0.020638	2.303824
105.806173	1681.508520	5.317222	-0.020694	2.308808
106.105751	1689.593535	5.322227	-0.020755	2.313781
106.465411	1697.623467	5.327232	-0.020828	2.318715
106.679101	1705.711202	5.332237	-0.020873	2.323661
106.820819	1713.781424	5.337242	-0.020904	2.328580
107.412330	1721.833089	5.342246	-0.021020	2.333515
107.663590	1729.922396	5.347251	-0.021072	2.338434
107.990404	1737.976510	5.352256	-0.021138	2.343327
108.257778	1746.066892	5.357261	-0.021193	2.348228
108.693125	1754.137869	5.362266	-0.021279	2.353119
109.138593	1762.187886	5.367270	-0.021368	2.357989
109.177509	1770.276859	5.372275	-0.021380	2.362839
109.392281	1778.325085	5.377280	-0.021425	2.367669
109.848633	1786.401647	5.382285	-0.021516	2.372526
109.971775	1794.457455	5.387290	-0.021544	2.377333
110.426911	1802.503262	5.392294	-0.021634	2.382152
110.619114	1810.581138	5.397299	-0.021675	2.386958
110.801950	1818.672200	5.402304	-0.021714	2.391762
111.380012	1826.707825	5.407309	-0.021827	2.396554
111.548560	1834.762599	5.412314	-0.021864	2.401316
111.867858	1842.830669	5.417318	-0.021928	2.406089
112.250322	1850.891143	5.422323	-0.022005	2.410852
112.624112	1858.953774	5.427328	-0.022080	2.415606
112.813699	1867.039871	5.432333	-0.022120	2.420350
113.004094	1875.099034	5.437338	-0.022161	2.425069
113.351123	1883.163513	5.442342	-0.022231	2.429794
113.489639	1891.346157	5.447347	-0.022262	2.434563
113.632311	1899.357272	5.452352	-0.022294	2.439223
114.136113	1907.367030	5.457357	-0.022393	2.443901
114.578326	1915.390563	5.462362	-0.022480	2.448573
114.913339	1923.465718	5.467366	-0.022548	2.453258
115.188980	1931.521988	5.472371	-0.022605	2.457918
115.404901	1939.563492	5.477376	-0.022650	2.462557
115.590664	1947.655021	5.482381	-0.022690	2.467213
115.773730	1955.723298	5.487386	-0.022729	2.471846
116.271652	1963.764465	5.492390	-0.022827	2.476480
116.556260	1971.815072	5.497395	-0.022885	2.481093
116.559627	1979.888564	5.502400	-0.022891	2.485691
117.171260	1987.915467	5.507405	-0.023010	2.490298
117.294145	1996.010992	5.512410	-0.023039	2.494900
117.448002	2004.067605	5.517414	-0.023072	2.499473
117.810142	2012.114962	5.522419	-0.023145	2.504048
117.938520	2020.190507	5.527424	-0.023174	2.508614
118.248822	2028.284354	5.532429	-0.023237	2.513194
118.476637	2036.329560	5.537434	-0.023285	2.517733
118.658908	2044.374395	5.542438	-0.023324	2.522260
119.125059	2052.416969	5.547443	-0.023416	2.526799
119.358528	2060.448730	5.552448	-0.023465	2.531306
119.642564	2068.550652	5.557453	-0.023523	2.535848
120.020872	2076.574495	5.562458	-0.023599	2.540345
120.274598	2084.626973	5.567462	-0.023651	2.544841
120.501003	2092.700990	5.572467	-0.023699	2.549339
120.663187	2100.766270	5.577472	-0.023734	2.553819
121.139299	2108.799828	5.582477	-0.023828	2.558297
121.239537	2116.842693	5.587482	-0.023852	2.562745
121.486563	2124.885876	5.592486	-0.023903	2.567196
121.563772	2132.981351	5.597491	-0.023923	2.571656
121.921049	2141.007027	5.602496	-0.023995	2.576089
122.068990	2149.081057	5.607501	-0.024027	2.580527
122.284024	2157.099015	5.612506	-0.024073	2.584931
122.615556	2165.148772	5.617510	-0.024140	2.589353
122.968738	2173.386489	5.622515	-0.024211	2.593871
123.283694	2181.385379	5.627520	-0.024275	2.598249
123.622109	2189.388710	5.632525	-0.024343	2.602623
123.905386	2197.385240	5.637530	-0.024401	2.606982
124.294567	2205.412723	5.642534	-0.024479	2.611358
124.686410	2213.476689	5.647539	-0.024557	2.615747
124.773090	2221.512142	5.652544	-0.024578	2.620092
125.192111	2229.539557	5.657549	-0.024661	2.624448
125.349661	2237.600114	5.662554	-0.024696	2.628797
125.618028	2245.676437	5.667558	-0.024751	2.633154
125.747712	2253.742041	5.672563	-0.024781	2.637490
126.138487	2261.740752	5.677568	-0.024859	2.641799
126.238609	2269.824107	5.682573	-0.024883	2.646128
126.463206	2277.856921	5.687578	-0.024930	2.650431
126.674538	2285.929764	5.692582	-0.024974	2.654747
126.870298	2293.983135	5.697587	-0.025016	2.659045
127.161465	2301.993314	5.702592	-0.025075	2.663319
127.446007	2310.040322	5.707597	-0.025134	2.667605
127.526020	2318.131820	5.712602	-0.025154	2.671894
128.077857	2326.173163	5.717606	-0.025262	2.676181
128.219099	2334.211215	5.722611	-0.025293	2.680433
128.449011	2342.207510	5.727616	-0.025341	2.684661
128.967543	2350.243430	5.732621	-0.025443	2.688922
128.991634	2358.346719	5.737626	-0.025453	2.693180
129.567076	2366.354132	5.742630	-0.025565	2.697416
129.996474	2374.388461	5.747635	-0.025651	2.701650
130.067795	2382.448171	5.752640	-0.025669	2.705868
130.272931	2390.524816	5.757645	-0.025713	2.710097
130.461619	2398.599985	5.762650	-0.025753	2.714317
130.997174	2406.588747	5.767654	-0.025858	2.718508
131.237883	2414.651788	5.772659	-0.025908	2.722712
131.355169	2422.692750	5.777664	-0.025935	2.726890
131.673180	2430.746984	5.782669	-0.026000	2.731081
131.916326	2438.817233	5.787674	-0.026050	2.735270
132.027081	2446.867888	5.792678	-0.026076	2.739434
132.416035	2454.881584	5.797683	-0.026154	2.743589
132.394464	2462.954333	5.802688	-0.026155	2.747744
132.689562	2471.069421	5.807693	-0.026215	2.751933
132.963732	2479.145334	5.812698	-0.026271	2.756094
133.226834	2487.120296	5.817702	-0.026326	2.760197
133.394435	2495.134972	5.822707	-0.026362	2.764308
133.688666	2503.138286	5.827712	-0.026422	2.768414
134.313975	2511.168827	5.832717	-0.026544	2.772548
134.882853	2519.202973	5.837722	-0.026655	2.776675
135.174164	2527.235685	5.842726	-0.026714	2.780778
135.667894	2535.261798	5.847731	-0.026811	2.784883
135.818761	2543.330632	5.852736	-0.026845	2.788984
135.926823	2551.436143	5.857741	-0.026870	2.793095
136.166420	2559.464903	5.862746	-0.026920	2.797168
136.411579	2567.494965	5.867750	-0.026971	2.801237
136.683107	2575.521409	5.872755	-0.027027	2.805299
136.770360	2583.561637	5.877760	-0.027048	2.809352
137.037035	2591.649453	5.882765	-0.027103	2.813433
137.111191	2599.692850	5.887770	-0.027122	2.817475
137.336963	2607.726728	5.892774	-0.027170	2.821515
137.637740	2615.757429	5.897779	-0.027231	2.825551
137.885887	2623.794548	5.902784	-0.027282	2.829582
138.242511	2631.887245	5.907789	-0.027354	2.833642
138.643004	2639.871409	5.912794	-0.027434	2.837643
138.942094	2647.893662	5.917798	-0.027495	2.841653
138.926730	2655.970635	5.922803	-0.027497	2.845666
139.092856	2663.991237	5.927808	-0.027533	2.849655
139.483730	2672.058923	5.932813	-0.027611	2.853675
139.552582	2680.109524	5.937818	-0.027629	2.857663
139.790274	2688.132162	5.942822	-0.027679	2.861641
140.280795	2696.143362	5.947827	-0.027775	2.865621
140.717271	2704.157464	5.952832	-0.027862	2.869595
140.929121	2712.250632	5.957837	-0.027907	2.873589
141.006430	2720.287589	5.962842	-0.027926	2.877543
141.240569	2728.318769	5.967846	-0.027975	2.881497
141.514094	2736.350987	5.972851	-0.028031	2.885448
141.459855	2744.404676	5.977856	-0.028026	2.889386
141.968649	2752.468146	5.982861	-0.028126	2.893355
142.295227	2760.485084	5.987866	-0.028192	2.897285
142.678612	2768.521546	5.992870	-0.028269	2.901222
143.021706	2776.561397	5.997875	-0.028338	2.905154
143.076252	2784.619740	6.002880	-0.028354	2.909074
143.290021	2792.763494	6.007885	-0.028399	2.913038
143.388746	2800.782231	6.012890	-0.028422	2.916930
143.598868	2808.785316	6.017894	-0.028467	2.920815
143.840411	2816.789274	6.022899	-0.028517	2.924698
144.089420	2824.778597	6.027904	-0.028568	2.928568
144.340938	2832.871012	6.032909	-0.028621	2.932483
144.737527	2840.881368	6.037914	-0.028700	2.936361
144.852210	2848.902659	6.042918	-0.028726	2.940224
145.296326	2856.923522	6.047923	-0.028814	2.944099
145.462512	2864.975546	6.052928	-0.028850	2.947969
145.490133	2873.069543	6.057933	-0.028861	2.951848
145.628441	2881.111313	6.062938	-0.028892	2.955701
145.932804	2889.105214	6.067942	-0.028954	2.959536
146.114654	2897.154264	6.072947	-0.028993	2.963385
146.271139	2905.152352	6.077952	-0.029027	2.967204
146.561477	2913.208853	6.082957	-0.029086	2.971053
146.994782	2921.249489	6.087962	-0.029172	2.974896
147.190911	2929.260927	6.092966	-0.029214	2.978708
147.290047	2937.326693	6.097971	-0.029238	2.982536
147.596433	2945.337931	6.102976	-0.029300	2.986344
147.898533	2953.375876	6.107981	-0.029362	2.990160
148.240057	2961.463741	6.112986	-0.029430	2.993996
148.517410	2969.476212	6.117990	-0.029487	2.997788
149.001846	2977.485729	6.122995	-0.029583	3.001584
149.319902	2985.470723	6.128000	-0.029647	3.005356
149.485078	2993.545851	6.133005	-0.029683	3.009158
149.575168	3001.602551	6.138010	-0.029705	3.012942
149.881450	3009.643433	6.143014	-0.029767	3.016725
150.181563	3017.683873	6.148019	-0.029829	3.020503
150.332580	3025.706007	6.153024	-0.029862	3.024260
150.667458	3033.757844	6.158029	-0.029930	3.028035
150.791221	3041.819772	6.163034	-0.029958	3.031800
151.030310	3049.859016	6.168038	-0.030008	3.035555
151.392898	3057.860612	6.173043	-0.030080	3.039294
151.379128	3065.897757	6.178048	-0.030083	3.043026
151.802132	3073.928606	6.183053	-0.030167	3.046772
151.926662	3081.958539	6.188058	-0.030195	3.050499
152.036047	3090.011396	6.193062	-0.030221	3.054231
152.239931	3098.048917	6.198067	-0.030264	3.057956
152.464563	3106.057007	6.203072	-0.030311	3.061664
152.764208	3114.088930	6.208077	-0.030372	3.065381
152.886554	3122.144124	6.213082	-0.030400	3.069097
153.100119	3130.241280	6.218086	-0.030445	3.072831
153.295814	3138.301944	6.223091	-0.030487	3.076544
153.318053	3146.279096	6.228096	-0.030496	3.080205
153.545551	3154.302892	6.233101	-0.030544	3.083893
154.000520	3162.306582	6.238106	-0.030634	3.087578
154.184887	3170.343977	6.243110	-0.030674	3.091262
154.251681	3178.409747	6.248115	-0.030691	3.094948
154.332933	3186.431671	6.253120	-0.030712	3.098611
154.724901	3194.444975	6.258125	-0.030790	3.102279
154.882219	3202.485986	6.263130	-0.030824	3.105946
155.219882	3210.486937	6.268134	-0.030892	3.109597
155.320516	3218.596131	6.273139	-0.030917	3.113283
155.340043	3226.599750	6.278144	-0.030925	3.116913
155.749865	3234.620824	6.283149	-0.031007	3.120564
156.172480	3242.628139	6.288154	-0.031091	3.124206
156.207146	3250.644020	6.293158	-0.031103	3.127829
156.444082	3258.721911	6.298163	-0.031152	3.131485
156.644009	3266.740949	6.303168	-0.031194	3.135109
157.040246	3274.758377	6.308173	-0.031273	3.138736
157.225843	3282.788613	6.313178	-0.031313	3.142356
157.435684	3290.808446	6.318182	-0.031357	3.145968
157.697492	3298.868726	6.323187	-0.031411	3.149596
157.903572	3306.911122	6.328192	-0.031455	3.153209
157.947330	3314.979370	6.333197	-0.031468	3.156823
158.281609	3322.966461	6.338202	-0.031536	3.160409
158.426963	3330.974839	6.343206	-0.031568	3.163992
158.651667	3339.037205	6.348211	-0.031615	3.167599
158.783796	3347.058943	6.353216	-0.031645	3.171179
159.191208	3355.117301	6.358221	-0.031726	3.174783
159.403893	3363.132813	6.363226	-0.031771	3.178356
159.600603	3371.150552	6.368230	-0.031813	3.181925
159.814463	3379.170823	6.373235	-0.031858	3.185492
160.120581	3387.183614	6.378240	-0.031920	3.189055
160.330175	3395.277558	6.383245	-0.031965	3.192647
160.937290	3403.285610	6.388250	-0.032083	3.196213
160.923512	3411.291230	6.393254	-0.032085	3.199747
161.277169	3419.333144	6.398259	-0.032157	3.203310
161.437701	3427.346479	6.403264	-0.032192	3.206847
161.543472	3435.421477	6.408269	-0.032217	3.210406
161.724733	3443.470662	6.413274	-0.032256	3.213952
161.981135	3451.484773	6.418278	-0.032309	3.217482
162.326088	3459.517303	6.423283	-0.032378	3.221020
162.450698	3467.501794	6.428288	-0.032406	3.224524
162.661205	3475.563363	6.433293	-0.032451	3.228061
162.949274	3483.609497	6.438298	-0.032510	3.231591
163.205096	3491.691900	6.443302	-0.032563	3.235131
163.203154	3499.729207	6.448307	-0.032568	3.238637
163.479467	3507.687057	6.453312	-0.032624	3.242116
163.700954	3515.676610	6.458317	-0.032671	3.245603
163.780130	3523.715314	6.463322	-0.032691	3.249102
164.013376	3531.765785	6.468326	-0.032739	3.252609
164.426352	3539.828687	6.473331	-0.032822	3.256124
164.485642	3547.800375	6.478336	-0.032838	3.259581
164.930177	3555.836175	6.483341	-0.032926	3.263078
165.120027	3563.875211	6.488346	-0.032966	3.266563
165.193545	3571.906067	6.493350	-0.032985	3.270035
165.338629	3579.991824	6.498355	-0.033018	3.273531
165.557553	3587.991200	6.503360	-0.033064	3.276988
165.903677	3596.022425	6.508365	-0.033133	3.280460
166.012588	3604.042399	6.513370	-0.033159	3.283915
166.085862	3612.049381	6.518374	-0.033178	3.287359
166.452693	3620.107492	6.523379	-0.033251	3.290832
166.494432	3628.142326	6.528384	-0.033264	3.294279
166.726687	3636.169253	6.533389	-0.033313	3.297727
167.141285	3644.202986	6.538394	-0.033395	3.301181
167.435241	3652.183771	6.543398	-0.033455	3.304604
167.506643	3660.265215	6.548403	-0.033474	3.308058
167.455304	3668.325051	6.553408	-0.033469	3.311494
167.786342	3676.358599	6.558413	-0.033536	3.314930
168.246315	3684.340081	6.563418	-0.033627	3.318345
168.156406	3692.360199	6.568422	-0.033616	3.321753
168.473795	3700.352634	6.573427	-0.033680	3.325160
168.871010	3708.371434	6.578432	-0.033759	3.328578
169.203391	3716.429412	6.583437	-0.033826	3.332007
169.517163	3724.478308	6.588442	-0.033890	3.335427
169.753552	3732.469290	6.593446	-0.033939	3.338817
169.771261	3740.520820	6.598451	-0.033948	3.342220
169.894407	3748.541815	6.603456	-0.033976	3.345611
170.181545	3756.561976	6.608461	-0.034035	3.349005
170.537055	3764.602290	6.613466	-0.034106	3.352406
170.714517	3772.658897	6.618470	-0.034144	3.355803
170.950693	3780.669677	6.623475	-0.034193	3.359180
171.159446	3788.678353	6.628480	-0.034238	3.362552
171.474702	3796.715070	6.633485	-0.034301	3.365936
171.620569	3804.760368	6.638490	-0.034334	3.369314
171.742975	3812.768085	6.643494	-0.034362	3.372672
172.192075	3820.843375	6.648499	-0.034451	3.376067
172.221757	3828.831121	6.653504	-0.034462	3.379406
172.486323	3836.851761	6.658509	-0.034516	3.382765
172.820530	3844.897078	6.663514	-0.034584	3.386132
172.971341	3852.921821	6.668518	-0.034617	3.389482
173.148270	3861.025913	6.673523	-0.034655	3.392861
173.438581	3869.060306	6.678528	-0.034714	3.396213
173.482116	3877.053541	6.683533	-0.034728	3.399535
173.578853	3885.029856	6.688538	-0.034751	3.402849
173.892050	3893.033607	6.693542	-0.034814	3.406179
174.242253	3901.055836	6.698547	-0.034885	3.409514
174.382482	3909.076354	6.703552	-0.034916	3.412838
174.609474	3917.139887	6.708557	-0.034964	3.416180
174.903548	3925.154460	6.713562	-0.035024	3.419500
174.869566	3933.154052	6.718566	-0.035023	3.422800
175.005292	3941.222410	6.723571	-0.035053	3.426130
175.264819	3949.211927	6.728576	-0.035107	3.429429
175.504058	3957.275459	6.733581	-0.035156	3.432755
175.801392	3965.339146	6.738586	-0.035217	3.436079
176.176453	3973.265251	6.743590	-0.035292	3.439346
176.520564	3981.332553	6.748595	-0.035361	3.442667
176.442145	3989.400914	6.753600	-0.035352	3.445971
176.607870	3997.431304	6.758605	-0.035388	3.449264
176.907560	4005.457881	6.763610	-0.035449	3.452558
176.823871	4013.478795	6.768614	-0.035439	3.455832
177.199443	4021.483414	6.773619	-0.035514	3.459113
177.494861	4029.506828	6.778624	-0.035574	3.462395
177.877194	4037.511125	6.783629	-0.035651	3.465669
178.047465	4045.563865	6.788634	-0.035688	3.468953
178.216589	4053.603678	6.793638	-0.035724	3.472228
178.536478	4061.663807	6.798643	-0.035789	3.475513
178.777519	4069.613306	6.803648	-0.035839	3.478748
178.836973	4077.684008	6.808653	-0.035856	3.482023
179.153253	4085.648842	6.813658	-0.035920	3.485260
179.218677	4093.728130	6.818662	-0.035937	3.488533
179.631341	4101.771618	6.823667	-0.036019	3.491799
179.937398	4109.738396	6.828672	-0.036081	3.495027
180.199611	4117.772594	6.833677	-0.036135	3.498278
180.183648	4125.829830	6.838682	-0.036138	3.501527
180.302424	4133.793394	6.843686	-0.036165	3.504739
180.796859	4141.846220	6.848691	-0.036262	3.507996
180.845224	4149.893039	6.853696	-0.036277	3.511234
181.210236	4157.920605	6.858701	-0.036350	3.514470
181.323227	4165.968874	6.863706	-0.036376	3.517704
181.401057	4173.980571	6.868710	-0.036396	3.520920
181.498318	4181.975542	6.873715	-0.036419	3.524126
181.550601	4190.003121	6.878720	-0.036434	3.527341
181.882363	4198.043365	6.883725	-0.036501	3.530567
182.023797	4206.093826	6.888730	-0.036533	3.533788
182.199378	4214.111566	6.893734	-0.036571	3.536994
182.498652	4222.133602	6.898739	-0.036632	3.540202
182.643393	4230.130007	6.903744	-0.036664	3.543393
183.299493	4238.147103	6.908749	-0.036791	3.546604
183.658818	4246.212831	6.913754	-0.036863	3.549823
183.875835	4254.296674	6.918758	-0.036909	3.553042
183.860936	4262.364312	6.923763	-0.036912	3.556244
184.089820	4270.295131	6.928768	-0.036959	3.559397
184.367415	4278.305934	6.933773	-0.037016	3.562580
184.591342	4286.320898	6.938778	-0.037063	3.565760
184.775651	4294.337360	6.943782	-0.037103	3.568936
185.097430	4302.392838	6.948787	-0.037168	3.572130
185.085178	4310.415297	6.953792	-0.037171	3.575297
185.004810	4318.422934	6.958797	-0.037161	3.578454
185.482307	4326.450036	6.963802	-0.037255	3.581632
185.809157	4334.411378	6.968806	-0.037321	3.584777
185.901440	4342.504032	6.973811	-0.037344	3.587964
185.949084	4350.513409	6.978816	-0.037358	3.591114
186.344096	4358.551714	6.983821	-0.037437	3.594282
186.490836	4366.594460	6.988826	-0.037469	3.597443
186.668709	4374.578391	6.993830	-0.037508	3.600578
187.028080	4382.589872	6.998835	-0.037580	3.603727
187.004017	4390.611144	7.003840	-0.037580	3.606866
187.347350	4398.612464	7.008845	-0.037650	3.610004
187.743312	4406.667537	7.013850	-0.037729	3.613162
187.805797	4414.729435	7.018854	-0.037745	3.616311
187.998083	4422.712360	7.023859	-0.037786	3.619430
188.137376	4430.742059	7.028864	-0.037818	3.622563
188.386403	4438.748619	7.033869	-0.037869	3.625687
188.405218	4446.824879	7.038874	-0.037878	3.628830
188.565545	4454.862924	7.043878	-0.037913	3.631958
189.034393	4462.898576	7.048883	-0.038006	3.635091
189.271214	4470.863295	7.053888	-0.038055	3.638188
189.270000	4478.924699	7.058893	-0.038060	3.641313
189.683816	4486.893439	7.063898	-0.038142	3.644411
189.947179	4494.935997	7.068902	-0.038196	3.647530
190.232184	4502.959040	7.073907	-0.038255	3.650640
190.129034	4511.023698	7.078912	-0.038241	3.653753
190.482038	4518.997728	7.083917	-0.038312	3.656840
190.591425	4527.038963	7.088922	-0.038337	3.659945
190.722844	4535.065324	7.093926	-0.038367	3.663041
191.123003	4543.133906	7.098931	-0.038447	3.666158
191.131913	4551.120636	7.103936	-0.038454	3.669231
191.253140	4559.169901	7.108941	-0.038482	3.672328
191.677480	4567.200820	7.113946	-0.038566	3.675423
191.923827	4575.179789	7.118950	-0.038617	3.678491
192.250753	4583.257923	7.123955	-0.038683	3.681596
192.270072	4591.219975	7.128960	-0.038692	3.684647
192.595079	4599.240192	7.133965	-0.038758	3.687725
192.855616	4607.278056	7.138970	-0.038811	3.690805
192.889384	4615.322166	7.143974	-0.038823	3.693880
193.219146	4623.383828	7.148979	-0.038889	3.696966
193.420165	4631.326533	7.153984	-0.038932	3.700001
193.520452	4639.340613	7.158989	-0.038956	3.703058
193.847932	4647.365439	7.163994	-0.039022	3.706122
194.234980	4655.388269	7.168998	-0.039100	3.709185
194.574021	4663.478519	7.174003	-0.039168	3.712269
194.596936	4671.550829	7.179008	-0.039177	3.715336
194.934435	4679.486165	7.184013	-0.039245	3.718356
195.292570	4687.536315	7.189018	-0.039317	3.721418
195.137248	4695.476901	7.194022	-0.039294	3.724423
195.375316	4703.545596	7.199027	-0.039343	3.727484
195.696860	4711.522442	7.204032	-0.039408	3.730509
195.720414	4719.610718	7.209037	-0.039418	3.733567
195.948375	4727.670408	7.214042	-0.039466	3.736617
196.060589	4735.607523	7.219046	-0.039492	3.739615
196.166282	4743.689793	7.224051	-0.039517	3.742665
196.268940	4751.658704	7.229056	-0.039541	3.745670
196.580676	4759.690712	7.234061	-0.039604	3.748701
196.736553	4767.768947	7.239066	-0.039639	3.751744
196.739207	4775.776891	7.244070	-0.039644	3.754754
196.967587	4783.803104	7.249075	-0.039692	3.757773
197.231028	4791.789607	7.254080	-0.039746	3.760776
197.331925	4799.790098	7.259085	-0.039770	3.763778
197.505599	4807.850928	7.264090	-0.039808	3.766802
197.851761	4815.837714	7.269094	-0.039878	3.769800
198.000391	4823.905652	7.274099	-0.039911	3.772821
198.120777	4831.936716	7.279104	-0.039938	3.775826
198.325148	4839.962471	7.284109	-0.039981	3.778827
198.459725	4847.973798	7.289114	-0.040012	3.781820
198.502336	4855.972765	7.294118	-0.040025	3.784803
198.732581	4863.986122	7.299123	-0.040073	3.787794
198.963908	4872.038576	7.304128	-0.040121	3.790797
199.201782	4880.095455	7.309133	-0.040171	3.793799
199.600950	4888.113976	7.314138	-0.040250	3.796788
199.850334	4896.056174	7.319142	-0.040302	3.799743
200.035176	4904.077484	7.324147	-0.040342	3.802723
200.013728	4912.096221	7.329152	-0.040343	3.805696
200.365627	4920.094335	7.334157	-0.040414	3.808667
200.743252	4928.185939	7.339162	-0.040489	3.811671
200.675954	4936.190891	7.344166	-0.040482	3.814630
200.887033	4944.253522	7.349171	-0.040527	3.817615
201.056203	4952.227730	7.354176	-0.040563	3.820564
201.361612	4960.196113	7.359181	-0.040625	3.823511
201.397689	4968.276843	7.364186	-0.040637	3.826491
201.543891	4976.271149	7.369190	-0.040670	3.829440
202.005405	4984.306334	7.374195	-0.040761	3.832408
202.082401	4992.320528	7.379200	-0.040780	3.835358
202.411258	5000.333492	7.384205	-0.040847	3.838311
202.578209	5008.384003	7.389210	-0.040883	3.841271
202.791173	5016.346322	7.394214	-0.040928	3.844198
202.888624	5024.429420	7.399219	-0.040952	3.847165
203.173528	5032.402679	7.404224	-0.041010	3.850092
203.515673	5040.466805	7.409229	-0.041079	3.853052
203.722185	5048.531993	7.414234	-0.041122	3.856008
203.805247	5056.504353	7.419238	-0.041143	3.858924
204.100722	5064.548903	7.424243	-0.041203	3.861869
204.243163	5072.525126	7.429248	-0.041235	3.864784
204.365670	5080.583012	7.434253	-0.041263	3.867726
204.674261	5088.618981	7.439258	-0.041326	3.870661
204.708278	5096.838990	7.444262	-0.041338	3.873656
205.033470	5104.862587	7.449267	-0.041403	3.876582
205.176610	5112.717547	7.454272	-0.041435	3.879442
205.185444	5120.741125	7.459277	-0.041442	3.882358
205.387780	5128.734610	7.464282	-0.041485	3.885264
205.602747	5136.704237	7.469286	-0.041530	3.888160
205.953965	5144.751066	7.474291	-0.041601	3.891085
206.214269	5152.780462	7.479296	-0.041654	3.893999
206.196439	5160.821141	7.484301	-0.041656	3.896909
206.661362	5168.802805	7.489306	-0.041748	3.899806
206.535215	5176.839629	7.494310	-0.041730	3.902708
206.643585	5184.838194	7.499315	-0.041755	3.905600
206.907631	5192.850242	7.504320	-0.041810	3.908497
207.134069	5200.896275	7.509325	-0.041857	3.911403
207.370442	5208.970415	7.514330	-0.041906	3.914317
207.358087	5216.921212	7.519334	-0.041909	3.917181
207.789042	5224.907256	7.524339	-0.041995	3.920062
207.971370	5232.954574	7.529344	-0.042034	3.922960
207.990396	5240.944065	7.534349	-0.042043	3.925831
208.307206	5248.989618	7.539354	-0.042107	3.928726
208.318487	5257.013963	7.544358	-0.042114	3.931605
208.572941	5265.060765	7.549363	-0.042167	3.934495
208.799852	5273.083592	7.554368	-0.042214	3.937373
209.049042	5281.062435	7.559373	-0.042266	3.940234
209.164796	5289.077368	7.564378	-0.042293	3.943104
209.280411	5297.086845	7.569382	-0.042320	3.945969
209.507551	5305.137812	7.574387	-0.042367	3.948849
209.762785	5313.186387	7.579392	-0.042420	3.951727
209.737062	5321.232748	7.584397	-0.042420	3.954596
210.078568	5329.243468	7.589402	-0.042489	3.957458
210.395900	5337.158718	7.594406	-0.042553	3.960283
210.606591	5345.220023	7.599411	-0.042598	3.963155
210.689874	5353.211721	7.604416	-0.042619	3.965999
210.803614	5361.251679	7.609421	-0.042645	3.968859
210.908140	5369.326949	7.614426	-0.042670	3.971728
211.140954	5377.302593	7.619430	-0.042718	3.974563
211.239110	5385.386378	7.624435	-0.042742	3.977431
211.367110	5393.353030	7.629440	-0.042771	3.980257
211.665258	5401.386232	7.634445	-0.042832	3.983107
211.751493	5409.399009	7.639450	-0.042853	3.985944
212.000314	5417.438256	7.644454	-0.042904	3.988791
212.156806	5425.449622	7.649459	-0.042939	3.991624
212.671874	5433.494479	7.654464	-0.043040	3.994473
212.868746	5441.551916	7.659469	-0.043082	3.997320
212.776457	5449.499949	7.664474	-0.043070	4.000121
212.941182	5457.542889	7.669478	-0.043106	4.002957
213.260802	5465.552674	7.674483	-0.043171	4.005783
213.549172	5473.568776	7.679488	-0.043229	4.008608
213.501531	5481.604840	7.684493	-0.043226	4.011433
213.745527	5489.671757	7.689498	-0.043277	4.014271
213.908218	5497.667163	7.694502	-0.043312	4.017081
214.136418	5505.688486	7.699507	-0.043360	4.019898
214.244777	5513.712805	7.704512	-0.043385	4.022714
214.380324	5521.723777	7.709517	-0.043416	4.025522
214.672088	5529.765699	7.714522	-0.043475	4.028343
214.667080	5537.762019	7.719526	-0.043479	4.031140
214.899767	5545.916185	7.724531	-0.043528	4.033995
215.001738	5553.894146	7.729536	-0.043552	4.036784
215.345191	5561.749241	7.734541	-0.043621	4.039531
215.577964	5569.833865	7.739546	-0.043670	4.042355
215.617412	5577.800789	7.744550	-0.043683	4.045134
215.944929	5585.852456	7.749555	-0.043749	4.047944
215.909653	5593.881188	7.754560	-0.043747	4.050739
216.324267	5601.884032	7.759565	-0.043830	4.053529
216.399706	5609.942653	7.764570	-0.043849	4.056332
216.445881	5617.881361	7.769574	-0.043863	4.059091
216.866115	5625.925169	7.774579	-0.043946	4.061890
217.173210	5633.875849	7.779584	-0.044009	4.064653
217.164757	5641.943175	7.784589	-0.044013	4.067450
217.324727	5649.974942	7.789594	-0.044048	4.070235
217.630326	5658.016301	7.794598	-0.044110	4.073023
217.904180	5666.055561	7.799603	-0.044166	4.075809
218.190273	5674.048467	7.804608	-0.044224	4.078577
218.128577	5682.050886	7.809613	-0.044218	4.081341
218.292109	5690.067844	7.814618	-0.044254	4.084111
218.317542	5698.079494	7.819622	-0.044264	4.086876
218.603675	5706.090849	7.824627	-0.044322	4.089642
218.797572	5714.137652	7.829632	-0.044364	4.092418
218.737044	5722.165464	7.834637	-0.044358	4.095182
218.999182	5730.206128	7.839642	-0.044412	4.097952
219.119238	5738.174283	7.844646	-0.044439	4.100694
219.409950	5746.187620	7.849651	-0.044499	4.103451
219.448201	5754.219762	7.854656	-0.044511	4.106210
219.722394	5762.229247	7.859661	-0.044567	4.108963
220.142880	5770.306077	7.864666	-0.044651	4.111738
220.188247	5778.333409	7.869670	-0.044664	4.114490
220.414701	5786.344771	7.874675	-0.044712	4.117237
220.692462	5794.323174	7.879680	-0.044769	4.119971
220.757036	5802.349595	7.884685	-0.044786	4.122717
220.865495	5810.375216	7.889690	-0.044811	4.125462
220.873334	5818.376093	7.894694	-0.044818	4.128195
221.144617	5826.431230	7.899699	-0.044874	4.130948
220.986066	5834.470830	7.904704	-0.044850	4.133688
221.208829	5842.503783	7.909709	-0.044896	4.136429
221.630680	5850.504768	7.914714	-0.044980	4.139160
221.714046	5858.514124	7.919718	-0.045001	4.141888
221.791451	5866.512489	7.924723	-0.045020	4.144610
221.991908	5874.555900	7.929728	-0.045063	4.147347
222.487298	5882.541969	7.934733	-0.045160	4.150066
222.761482	5890.591798	7.939738	-0.045217	4.152802
222.769722	5898.620392	7.944742	-0.045224	4.155527
222.986971	5906.626789	7.949747	-0.045269	4.158244
222.947859	5914.643632	7.954752	-0.045267	4.160960
223.168354	5922.606122	7.959757	-0.045313	4.163659
223.296258	5930.667456	7.964762	-0.045343	4.166389
223.571957	5938.628496	7.969766	-0.045399	4.169084
223.845881	5946.692816	7.974771	-0.045455	4.171813
224.406562	5954.752050	7.979776	-0.045565	4.174541
224.516316	5962.759573	7.984781	-0.045591	4.177245
224.462181	5970.764775	7.989786	-0.045586	4.179945
224.597653	5978.752250	7.994790	-0.045616	4.182639
225.199412	5986.729751	7.999795	-0.045733	4.185333
225.308111	5994.799111	8.004800	-0.045759	4.188051
225.312364	6002.814003	8.009805	-0.045765	4.190747
225.626262	6010.939345	8.014810	-0.045829	4.193482
225.628236	6018.976869	8.019814	-0.045834	4.196183
225.662184	6026.920909	8.024819	-0.045846	4.198850
225.939119	6034.933126	8.029824	-0.045903	4.201542
226.124379	6042.857538	8.034829	-0.045942	4.204201
226.180465	6050.943885	8.039834	-0.045958	4.206912
226.473779	6058.894822	8.044838	-0.046018	4.209578
226.640026	6066.981716	8.049843	-0.046054	4.212286
226.709592	6074.981596	8.054848	-0.046072	4.214962
226.771457	6083.011121	8.059853	-0.046089	4.217647
227.264335	6090.988908	8.064858	-0.046186	4.220317
227.394355	6098.992139	8.069862	-0.046215	4.222990
227.529915	6107.006890	8.074867	-0.046246	4.225665
227.728332	6115.079259	8.079872	-0.046288	4.228359
227.778392	6123.038420	8.084877	-0.046303	4.231011
228.003727	6131.174768	8.089882	-0.046350	4.233723
227.913628	6139.148164	8.094886	-0.046338	4.236375
228.180959	6147.135061	8.099891	-0.046393	4.239034
228.445880	6155.136554	8.104896	-0.046448	4.241696
228.547759	6163.088563	8.109901	-0.046472	4.244338
228.927426	6171.188309	8.114906	-0.046548	4.247030
228.917050	6179.176199	8.119910	-0.046551	4.249679
228.993111	6187.266540	8.124915	-0.046571	4.252362
229.250761	6195.257114	8.129920	-0.046624	4.255012
229.760596	6203.255327	8.134925	-0.046724	4.257665
229.793351	6211.278285	8.139930	-0.046735	4.260320
229.941146	6219.307893	8.144934	-0.046768	4.262976
230.033160	6227.301542	8.149939	-0.046790	4.265619
230.184432	6235.385617	8.154944	-0.046824	4.268290
230.102340	6243.384458	8.159949	-0.046814	4.270929
230.467086	6251.465540	8.164954	-0.046887	4.273598
230.739429	6259.450013	8.169958	-0.046943	4.276232
230.721448	6267.417616	8.174963	-0.046945	4.278857
231.093506	6275.453183	8.179968	-0.047019	4.281505
231.351534	6283.425589	8.184973	-0.047072	4.284131
231.339215	6291.504775	8.189978	-0.047075	4.286787
231.233105	6299.434513	8.194982	-0.047061	4.289392
231.452461	6307.534988	8.199987	-0.047107	4.292054
231.689344	6315.530735	8.204992	-0.047156	4.294681
231.782668	6323.576872	8.209997	-0.047179	4.297321
231.996990	6331.573631	8.215002	-0.047224	4.299944
232.081965	6339.594676	8.220006	-0.047245	4.302572
232.414821	6347.588060	8.225011	-0.047312	4.305192
232.544709	6355.614152	8.230016	-0.047342	4.307819
232.658655	6363.658948	8.235021	-0.047368	4.310451
232.890672	6371.705016	8.240026	-0.047417	4.313082
232.855624	6379.676190	8.245030	-0.047415	4.315685
232.869691	6387.701758	8.250035	-0.047423	4.318305
232.935022	6395.721479	8.255040	-0.047441	4.320921
233.081526	6403.678175	8.260045	-0.047473	4.323516
233.240767	6411.716115	8.265050	-0.047508	4.326136
233.507248	6419.750881	8.270054	-0.047563	4.328754
233.535410	6427.768963	8.275059	-0.047573	4.331364
233.608596	6435.819733	8.280064	-0.047592	4.333982
233.797012	6443.793184	8.285069	-0.047632	4.336575
233.950659	6451.812610	8.290074	-0.047666	4.339181
233.856256	6459.818104	8.295078	-0.047654	4.341779
234.250647	6467.790239	8.300083	-0.047733	4.344368
234.451620	6475.881100	8.305088	-0.047775	4.346993
234.672980	6483.873399	8.310093	-0.047822	4.349584
234.599293	6491.925731	8.315098	-0.047813	4.352191
234.868338	6499.999138	8.320102	-0.047869	4.354806
235.119203	6508.034426	8.325107	-0.047921	4.357407
235.367067	6515.961650	8.330112	-0.047972	4.359971
235.588759	6523.933791	8.335117	-0.048018	4.362548
235.548039	6531.961273	8.340122	-0.048016	4.365139
235.739125	6539.972629	8.345126	-0.048057	4.367726
235.863996	6547.994914	8.350131	-0.048085	4.370313
235.975048	6556.028084	8.355136	-0.048111	4.372903
236.073631	6564.023639	8.360141	-0.048135	4.375479
236.322550	6572.060969	8.365146	-0.048186	4.378068
236.489146	6580.048357	8.370150	-0.048223	4.380638
236.476997	6588.064120	8.375155	-0.048226	4.383216
236.520251	6596.126379	8.380160	-0.048239	4.385807
236.859019	6604.122112	8.385165	-0.048307	4.388376
237.079250	6612.167547	8.390170	-0.048353	4.390960
237.026372	6620.172857	8.395174	-0.048349	4.393527
237.213847	6628.190442	8.400179	-0.048389	4.396099
237.557159	6636.205312	8.405184	-0.048458	4.398668
237.475542	6644.233044	8.410189	-0.048448	4.401238
237.679458	6652.209037	8.415194	-0.048491	4.403792
237.804578	6660.234965	8.420198	-0.048520	4.406359
238.052127	6668.282234	8.425203	-0.048571	4.408933
238.130240	6676.325262	8.430208	-0.048591	4.411503
238.258009	6684.297901	8.435213	-0.048620	4.414049
238.277777	6692.401168	8.440218	-0.048629	4.416634
238.285211	6700.323319	8.445222	-0.048635	4.419161
238.465209	6708.373820	8.450227	-0.048674	4.421727
238.644640	6716.391829	8.455232	-0.048713	4.424282
238.741460	6724.374560	8.460237	-0.048736	4.426823
238.988546	6732.449076	8.465242	-0.048787	4.429394
239.175644	6740.454599	8.470246	-0.048827	4.431940
239.381412	6748.507785	8.475251	-0.048871	4.434500
239.493525	6756.537516	8.480256	-0.048897	4.437051
239.557363	6764.444676	8.485261	-0.048914	4.439561
239.900604	6772.547493	8.490266	-0.048983	4.442133
240.091461	6780.467069	8.495270	-0.049024	4.444644
240.178102	6788.528581	8.500275	-0.049045	4.447199
240.359534	6796.513671	8.505280	-0.049084	4.449728
240.338703	6804.547395	8.510285	-0.049086	4.452271
240.495479	6812.608171	8.515290	-0.049120	4.454821
240.769912	6820.594147	8.520294	-0.049177	4.457347
240.873375	6828.587829	8.525299	-0.049201	4.459873
240.854955	6836.650841	8.530304	-0.049203	4.462419
241.117862	6844.614223	8.535309	-0.049257	4.464933
241.385003	6852.699979	8.540314	-0.049312	4.467484
241.424177	6860.678139	8.545318	-0.049325	4.470000
241.559194	6868.728142	8.550323	-0.049355	4.472536
241.762859	6876.738385	8.555328	-0.049398	4.475059
241.854930	6884.745505	8.560333	-0.049420	4.477579
242.188508	6892.719876	8.565338	-0.049488	4.480088
242.390432	6900.755858	8.570343	-0.049531	4.482615
242.536256	6908.727449	8.575347	-0.049563	4.485120
242.694665	6916.815827	8.580352	-0.049598	4.487660
242.589124	6924.785053	8.585357	-0.049583	4.490160
242.875545	6932.871429	8.590362	-0.049642	4.492697
242.955912	6940.831924	8.595367	-0.049662	4.495193
242.927877	6948.857691	8.600371	-0.049662	4.497707
243.261153	6956.850777	8.605376	-0.049729	4.500210
243.288157	6964.855146	8.610381	-0.049740	4.502715
243.464643	6972.898648	8.615386	-0.049778	4.505231
243.656571	6980.931608	8.620391	-0.049819	4.507742
243.774293	6988.937752	8.625395	-0.049846	4.510244
243.848431	6997.008759	8.630400	-0.049865	4.512764
243.905957	7005.020394	8.635405	-0.049881	4.515264
244.337176	7013.024630	8.640410	-0.049966	4.517761
244.350999	7020.962441	8.645415	-0.049974	4.520235
244.458497	7029.008190	8.650419	-0.049999	4.522742
244.634899	7037.000794	8.655424	-0.050037	4.525231
244.857827	7045.016624	8.660429	-0.050084	4.527726
245.261211	7053.046810	8.665434	-0.050164	4.530224
245.203052	7061.056455	8.670439	-0.050159	4.532713
245.397671	7069.083979	8.675443	-0.050200	4.535208
245.522423	7077.147611	8.680448	-0.050229	4.537711
245.317400	7085.073788	8.685453	-0.050196	4.540171
245.766847	7093.117259	8.690458	-0.050285	4.542666
245.904611	7101.093509	8.695463	-0.050316	4.545139
246.125280	7109.163437	8.700467	-0.050362	4.547639
246.251425	7117.218214	8.705472	-0.050391	4.550133
246.442068	7125.206510	8.710477	-0.050431	4.552606
246.483026	7133.288792	8.715482	-0.050444	4.555105
246.324376	7141.221873	8.720487	-0.050420	4.557557
246.646847	7149.173257	8.725491	-0.050485	4.560014
246.947499	7157.265686	8.730496	-0.050546	4.562514
246.884782	7165.215363	8.735501	-0.050540	4.564967
247.112910	7173.294763	8.740506	-0.050588	4.567459
247.475758	7181.297153	8.745511	-0.050660	4.569926
247.533362	7189.353697	8.750515	-0.050676	4.572409
247.696001	7197.378821	8.755520	-0.050712	4.574880
247.814668	7205.354709	8.760525	-0.050739	4.577335
247.976146	7213.389636	8.765530	-0.050775	4.579807
248.087345	7221.426057	8.770535	-0.050800	4.582277
248.373903	7229.375994	8.775539	-0.050859	4.584720
248.509943	7237.455698	8.780544	-0.050890	4.587202
248.572490	7245.425014	8.785549	-0.050906	4.589648
248.812536	7253.505181	8.790554	-0.050956	4.592127
248.875617	7261.546304	8.795559	-0.050973	4.594592
248.828240	7269.559324	8.800563	-0.050970	4.597048
249.019031	7277.497816	8.805568	-0.051011	4.599479
249.293615	7285.523137	8.810573	-0.051067	4.601936
249.526209	7293.524316	8.815578	-0.051115	4.604384
249.524448	7301.588214	8.820583	-0.051120	4.606849
249.754232	7309.561308	8.825587	-0.051168	4.609286
250.205527	7317.653168	8.830592	-0.051258	4.611758
250.308047	7325.639096	8.835597	-0.051282	4.614196
250.479242	7333.667173	8.840602	-0.051319	4.616645
250.444371	7341.640126	8.845607	-0.051318	4.619077
250.525434	7349.656269	8.850611	-0.051338	4.621520
250.756758	7357.698329	8.855616	-0.051386	4.623970
250.610582	7365.660301	8.860621	-0.051364	4.626394
250.795475	7373.734520	8.865626	-0.051404	4.628851
250.971450	7381.744305	8.870631	-0.051442	4.631287
251.117399	7389.762447	8.875635	-0.051474	4.633725
251.200133	7397.765239	8.880640	-0.051495	4.636156
251.450762	7405.710888	8.885645	-0.051547	4.638569
251.649180	7413.812949	8.890650	-0.051589	4.641028
251.845963	7421.783498	8.895655	-0.051631	4.643445
251.954881	7429.782788	8.900659	-0.051657	4.645870
252.161705	7437.811302	8.905664	-0.051700	4.648303
252.350987	7445.814159	8.910669	-0.051741	4.650727
252.520409	7453.892393	8.915674	-0.051778	4.653172
252.557419	7461.867172	8.920679	-0.051790	4.655584
252.792482	7469.889134	8.925683	-0.051839	4.658010
253.054288	7477.912375	8.930688	-0.051893	4.660435
253.262169	7485.893174	8.935693	-0.051937	4.662845
253.476869	7493.932005	8.940698	-0.051982	4.665272
253.544791	7501.929991	8.945703	-0.052000	4.667685
253.763916	7509.924536	8.950707	-0.052046	4.670096
253.903565	7518.035859	8.955712	-0.052077	4.672541
253.959339	7526.076459	8.960717	-0.052093	4.674963
254.064040	7534.083132	8.965722	-0.052117	4.677374
254.440438	7542.023804	8.970727	-0.052193	4.679763
254.529412	7550.062644	8.975731	-0.052214	4.682181
254.729671	7558.005552	8.980736	-0.052257	4.684569
254.557695	7566.033579	8.985741	-0.052230	4.686982
254.823005	7574.028790	8.990746	-0.052285	4.689382
254.764287	7582.108390	8.995751	-0.052279	4.691808
255.257149	7590.128018	9.000755	-0.052376	4.694213
255.250057	7598.150756	9.005760	-0.052380	4.696619
255.420589	7606.091293	9.010765	-0.052417	4.698998
255.489756	7614.153019	9.015770	-0.052435	4.701413
255.408851	7622.141714	9.020775	-0.052425	4.703805
255.592623	7630.184398	9.025779	-0.052465	4.706212
255.711792	7638.189028	9.030784	-0.052492	4.708606
255.754203	7646.200326	9.035789	-0.052505	4.711001
255.921773	7654.276289	9.040794	-0.052542	4.713413
256.184329	7662.279855	9.045799	-0.052596	4.715803
256.366067	7670.252393	9.050803	-0.052635	4.718182
256.367650	7678.289256	9.055808	-0.052640	4.720580
256.518253	7686.280195	9.060813	-0.052674	4.722962
256.875820	7694.324229	9.065818	-0.052745	4.725359
256.724482	7702.376248	9.070823	-0.052722	4.727758
256.978401	7710.317551	9.075827	-0.052775	4.730121
257.241307	7718.430920	9.080832	-0.052829	4.732535
257.248375	7726.367573	9.085837	-0.052836	4.734896
257.330514	7734.458106	9.090842	-0.052856	4.737300
257.543555	7742.394354	9.095847	-0.052901	4.739658
257.611787	7750.423589	9.100851	-0.052919	4.742042
257.736293	7758.422768	9.105856	-0.052947	4.744416
257.706691	7766.462262	9.110861	-0.052947	4.746801
258.052686	7774.481436	9.115866	-0.053017	4.749178
258.263214	7782.529614	9.120871	-0.053061	4.751563
258.295132	7790.567266	9.125875	-0.053072	4.753943
258.569240	7798.601190	9.130880	-0.053129	4.756321
258.565650	7806.476673	9.135885	-0.053133	4.758652
258.804370	7814.568988	9.140890	-0.053183	4.761044
259.002268	7822.610055	9.145895	-0.053225	4.763421
259.213072	7830.571887	9.150899	-0.053269	4.765773
259.346324	7838.617140	9.155904	-0.053299	4.768148
259.589052	7846.574747	9.160909	-0.053350	4.770496
259.857228	7854.701818	9.165914	-0.053405	4.772893
259.771621	7862.671759	9.170919	-0.053394	4.775244
259.840320	7870.634923	9.175923	-0.053412	4.777590
260.310938	7878.677377	9.180928	-0.053505	4.779958
260.184172	7886.677715	9.185933	-0.053487	4.782314
260.280169	7894.686087	9.190938	-0.053510	4.784671
260.534091	7902.746307	9.195943	-0.053562	4.787040
260.827393	7910.715591	9.200947	-0.053622	4.789382
260.899558	7918.773922	9.205952	-0.053641	4.791750
260.758744	7926.753436	9.210957	-0.053620	4.794094
261.101323	7934.790741	9.215962	-0.053689	4.796452
261.401448	7942.816607	9.220967	-0.053750	4.798806
261.562931	7950.775226	9.225971	-0.053785	4.801139
261.678931	7958.816987	9.230976	-0.053812	4.803496
261.573908	7966.787907	9.235981	-0.053798	4.805832
261.693147	7974.809919	9.240986	-0.053825	4.808181
261.890155	7982.843546	9.245991	-0.053867	4.810531
262.106272	7990.364878	9.250995	-0.053912	4.812731
262.245322	7994.942514	9.256000	-0.053941	4.814069
262.218359	7997.459835	9.261005	-0.053938	4.814805
262.595157	7998.856357	9.266010	-0.054009	4.815212
262.551395	7999.272143	9.271015	-0.054001	4.815333
262.539374	8000.214982	9.276019	-0.053999	4.815609
262.793707	8000.298173	9.281024	-0.054047	4.815632
262.985082	8000.307709	9.286029	-0.054082	4.815634
263.019096	8000.321082	9.291034	-0.054089	4.815638
263.108557	8000.346041	9.296039	-0.054106	4.815645
263.302424	8000.257359	9.301043	-0.054142	4.815618
263.290324	8000.339401	9.306048	-0.054139	4.815642
263.134482	8000.336854	9.311053	-0.054110	4.815642
263.394949	8000.321887	9.316058	-0.054159	4.815636
263.456317	8000.364545	9.321063	-0.054170	4.815648
263.199403	8000.249269	9.326067	-0.054122	4.815616
263.310099	8000.374972	9.331072	-0.054143	4.815652
263.498750	8000.369512	9.336077	-0.054178	4.815650
263.555514	8000.409958	9.341082	-0.054189	4.815661
263.456182	8000.384838	9.346087	-0.054170	4.815654
263.509690	8000.389985	9.351091	-0.054180	4.815656
263.451562	8000.351653	9.356096	-0.054169	4.815645
263.446416	8000.340889	9.361101	-0.054168	4.815641
263.713604	8000.314284	9.366106	-0.054218	4.815632
263.779735	8000.373041	9.371111	-0.054231	4.815649
263.707296	8000.269323	9.376115	-0.054217	4.815619
263.715267	8000.343150	9.381120	-0.054219	4.815641
263.730550	8000.311358	9.386125	-0.054221	4.815631
263.619385	8000.343719	9.391130	-0.054201	4.815641
263.626607	8000.339565	9.396135	-0.054202	4.815640
263.822218	8000.336356	9.401139	-0.054238	4.815638
263.993728	8000.332752	9.406144	-0.054270	4.815636
263.866239	8000.298626	9.411149	-0.054247	4.815627
263.969850	8000.255462	9.416154	-0.054266	4.815614
264.048181	8000.256743	9.421159	-0.054281	4.815614
263.752078	8000.290352	9.426163	-0.054225	4.815625
263.888159	8000.296850	9.431168	-0.054251	4.815626
263.975352	8000.311092	9.436173	-0.054267	4.815630
263.922452	8000.231192	9.441178	-0.054257	4.815607
264.006828	8000.316948	9.446183	-0.054273	4.815632
263.959097	8000.287330	9.451187	-0.054264	4.815623
263.982830	8000.311216	9.456192	-0.054268	4.815630
263.820252	8000.324579	9.461197	-0.054238	4.815635
264.077665	8000.298883	9.466202	-0.054286	4.815626
264.119115	8000.335875	9.471207	-0.054294	4.815637
263.970275	8000.316353	9.476211	-0.054266	4.815632
264.000869	8000.318990	9.481216	-0.054272	4.815632
264.041855	8000.256644	9.486221	-0.054279	4.815614
264.066299	8000.264521	9.491226	-0.054284	4.815616
264.244605	8000.257824	9.496231	-0.054317	4.815613
264.321024	8000.214215	9.501235	-0.054331	4.815600
264.349511	8000.227498	9.506240	-0.054337	4.815604
264.235760	8000.250204	9.511245	-0.054316	4.815611
264.124303	8000.306058	9.516250	-0.054295	4.815628
264.341066	8000.307467	9.521255	-0.054335	4.815627
264.274750	8000.318131	9.526259	-0.054323	4.815631
264.359526	8000.364377	9.531264	-0.054339	4.815644
264.332737	8000.369280	9.536269	-0.054334	4.815646
264.276174	8000.355538	9.541274	-0.054323	4.815642
264.334199	8000.372509	9.546279	-0.054334	4.815646
264.375436	8000.328324	9.551283	-0.054342	4.815633
264.593786	8000.325487	9.556288	-0.054382	4.815631
264.391774	8000.332865	9.561293	-0.054345	4.815635
264.415141	8000.364221	9.566298	-0.054349	4.815644
264.532659	8000.359735	9.571303	-0.054371	4.815642
264.305038	8000.370966	9.576307	-0.054329	4.815646
264.301972	8000.431797	9.581312	-0.054328	4.815664
264.335488	8000.385350	9.586317	-0.054334	4.815650
264.429339	8000.368728	9.591322	-0.054352	4.815645
264.337758	8000.344801	9.596327	-0.054335	4.815638
264.564390	8000.348508	9.601331	-0.054377	4.815638
264.768945	8000.372148	9.606336	-0.054415	4.815644
264.515120	8000.355179	9.611341	-0.054368	4.815641
264.318197	8000.278262	9.616346	-0.054331	4.815619
264.529156	8000.381043	9.621351	-0.054370	4.815648
264.398512	8000.312686	9.626355	-0.054346	4.815629
264.371300	8000.363509	9.631360	-0.054341	4.815644
264.283473	8000.359937	9.636365	-0.054325	4.815643
264.377466	8000.317684	9.641370	-0.054342	4.815630
264.354883	8000.318383	9.646375	-0.054338	4.815631
264.310303	8000.301633	9.651379	-0.054330	4.815626
264.407646	8000.350221	9.656384	-0.054348	4.815640
264.451136	8000.291120	9.661389	-0.054356	4.815622
264.430166	8000.265144	9.666394	-0.054352	4.815615
264.534845	8000.373664	9.671399	-0.054371	4.815646
264.520376	8000.316819	9.676403	-0.054369	4.815629
264.630533	8000.364549	9.681408	-0.054389	4.815643
264.666586	8000.334165	9.686413	-0.054396	4.815634
264.984514	8000.301982	9.691418	-0.054455	4.815623
264.897981	8000.362516	9.696423	-0.054439	4.815641
264.580512	8000.243040	9.701427	-0.054380	4.815607
264.749448	8000.368632	9.706432	-0.054411	4.815643
264.812604	8000.356849	9.711437	-0.054423	4.815640
264.648076	8000.350953	9.716442	-0.054393	4.815639
264.605730	8000.406869	9.721447	-0.054385	4.815655
264.911850	8000.364882	9.726451	-0.054442	4.815641
264.996503	8000.408991	9.731456	-0.054457	4.815654
264.711424	8000.391510	9.736461	-0.054404	4.815650
264.742897	8000.330077	9.741466	-0.054410	4.815632
264.966928	8000.373261	9.746471	-0.054452	4.815644
264.795098	8000.297821	9.751475	-0.054420	4.815622
264.980815	8000.382034	9.756480	-0.054455	4.815646
264.980870	8000.374558	9.761485	-0.054455	4.815644
264.755595	8000.359124	9.766490	-0.054413	4.815641
264.746205	8000.385673	9.771495	-0.054411	4.815648
264.822485	8000.314292	9.776499	-0.054425	4.815627
264.932500	8000.342794	9.781504	-0.054446	4.815635
264.823303	8000.314306	9.786509	-0.054425	4.815627
264.799538	8000.308577	9.791514	-0.054421	4.815626
265.046005	8000.408737	9.796519	-0.054467	4.815654
264.735070	8000.323545	9.801523	-0.054409	4.815630
264.917762	8000.343623	9.806528	-0.054443	4.815635
264.858942	8000.301006	9.811533	-0.054432	4.815623
264.742949	8000.298041	9.816538	-0.054410	4.815623
264.913861	8000.375603	9.821543	-0.054442	4.815645
265.066501	8000.321491	9.826547	-0.054471	4.815628
265.174686	8000.333943	9.831552	-0.054491	4.815631
264.872643	8000.357840	9.836557	-0.054434	4.815640
264.900306	8000.336931	9.841562	-0.054440	4.815633
264.968178	8000.370085	9.846567	-0.054452	4.815643
264.846257	8000.316822	9.851571	-0.054430	4.815628
265.011461	8000.325934	9.856576	-0.054460	4.815630
265.177949	8000.357496	9.861581	-0.054491	4.815638
265.214215	8000.273711	9.866586	-0.054498	4.815613
265.043356	8000.385202	9.871591	-0.054466	4.815647
264.939765	8000.371758	9.876595	-0.054447	4.815643
264.991859	8000.391837	9.881600	-0.054457	4.815649
264.897302	8000.394562	9.886605	-0.054439	4.815650
265.011610	8000.401773	9.891610	-0.054460	4.815652
264.872440	8000.411246	9.896615	-0.054435	4.815655
264.969536	8000.320979	9.901619	-0.054453	4.815628
265.093401	8000.404181	9.906624	-0.054476	4.815652
265.208659	8000.401794	9.911629	-0.054497	4.815651
264.919150	8000.400263	9.916634	-0.054443	4.815652
265.019412	8000.363452	9.921639	-0.054462	4.815641
265.109217	8000.349968	9.926643	-0.054479	4.815636
265.299193	8000.429980	9.931648	-0.054514	4.815659
264.984040	8000.374623	9.936653	-0.054455	4.815644
265.084235	8000.386944	9.941658	-0.054474	4.815647
265.075967	8000.354766	9.946663	-0.054472	4.815638
265.037221	8000.317818	9.951667	-0.054465	4.815627
265.028445	8000.393509	9.956672	-0.054464	4.815649
265.022916	8000.379534	9.961677	-0.054463	4.815645
265.210862	8000.283276	9.966682	-0.054498	4.815616
265.268671	8000.339763	9.971687	-0.054508	4.815632
265.114116	8000.373550	9.976691	-0.054480	4.815643
265.212560	8000.377297	9.981696	-0.054498	4.815644
264.987442	8000.421679	9.986701	-0.054456	4.815658
265.067353	8000.353561	9.991706	-0.054471	4.815637
265.294355	8000.408544	9.996711	-0.054513	4.815652
265.127017	8000.382308	10.001715	-0.054482	4.815646
265.296390	8000.412850	10.006720	-0.054514	4.815654
265.209015	8000.362288	10.011725	-0.054497	4.815639
265.238253	8000.310430	10.016730	-0.054503	4.815624
265.299303	8000.421444	10.021735	-0.054514	4.815656
265.309586	8000.351118	10.026739	-0.054516	4.815636
265.512656	8000.365122	10.031744	-0.054554	4.815639
265.224617	8000.407406	10.036749	-0.054500	4.815652
265.071088	8000.410234	10.041754	-0.054472	4.815654
265.219391	8000.397708	10.046759	-0.054499	4.815650
265.349012	8000.378467	10.051763	-0.054523	4.815643
265.420274	8000.400996	10.056768	-0.054537	4.815650
265.384006	8000.359815	10.061773	-0.054530	4.815638
265.509773	8000.431300	10.066778	-0.054553	4.815658
265.218774	8000.406244	10.071783	-0.054499	4.815652
265.250018	8000.372577	10.076787	-0.054505	4.815642
265.358581	8000.456598	10.081792	-0.054525	4.815666
265.176965	8000.385268	10.086797	-0.054491	4.815646
265.274125	8000.359087	10.091802	-0.054509	4.815638
265.256890	8000.426096	10.096807	-0.054506	4.815658
265.396219	8000.425172	10.101811	-0.054532	4.815657
265.331535	8000.433727	10.106816	-0.054520	4.815660
265.353659	8000.378548	10.111821	-0.054524	4.815643
265.372355	8000.426919	10.116826	-0.054528	4.815657
265.250405	8000.449490	10.121831	-0.054505	4.815665
265.328089	8000.411242	10.126835	-0.054520	4.815653
265.633959	8000.440814	10.131840	-0.054577	4.815660
265.496301	8000.415063	10.136845	-0.054551	4.815653
265.366798	8000.327496	10.141850	-0.054527	4.815628
265.290153	8000.444802	10.146855	-0.054513	4.815663
265.205940	8000.299231	10.151859	-0.054497	4.815621
265.319731	8000.401494	10.156864	-0.054518	4.815650
265.282494	8000.382728	10.161869	-0.054511	4.815645
265.574393	8000.354393	10.166874	-0.054565	4.815635
265.404614	8000.441336	10.171879	-0.054534	4.815661
265.340764	8000.353775	10.176883	-0.054522	4.815636
265.542258	8000.413682	10.181888	-0.054559	4.815653
265.415020	8000.427622	10.186893	-0.054536	4.815657
265.442742	8000.322334	10.191898	-0.054541	4.815626
265.524880	8000.388833	10.196903	-0.054556	4.815646
265.448628	8000.326703	10.201907	-0.054542	4.815628
265.495407	8000.435348	10.206912	-0.054551	4.815659
265.533691	8000.366548	10.211917	-0.054558	4.815639
265.580399	8000.360904	10.216922	-0.054567	4.815637
265.469728	8000.401817	10.221927	-0.054546	4.815650
265.370348	8000.360672	10.226931	-0.054527	4.815638
265.541375	8000.420080	10.231936	-0.054559	4.815655
265.620582	8000.380789	10.236941	-0.054574	4.815643
265.585871	8000.418673	10.241946	-0.054568	4.815654
265.572416	8000.386410	10.246951	-0.054565	4.815645
265.724686	8000.340837	10.251955	-0.054593	4.815631
265.655335	8000.410198	10.256960	-0.054581	4.815651
265.606743	8000.409403	10.261965	-0.054572	4.815651
265.671486	8000.363466	10.266970	-0.054584	4.815637
265.773414	8000.419608	10.271975	-0.054603	4.815653
265.396680	8000.338676	10.276979	-0.054532	4.815631
265.575064	8000.376843	10.281984	-0.054566	4.815642
265.485807	8000.384996	10.286989	-0.054549	4.815645
265.433285	8000.301893	10.291994	-0.054539	4.815621
265.670198	8000.414717	10.296999	-0.054583	4.815652
265.668816	8000.421103	10.302003	-0.054583	4.815654
265.752286	8000.436355	10.307008	-0.054599	4.815658
265.609700	8000.419068	10.312013	-0.054572	4.815654
265.570800	8000.358618	10.317018	-0.054565	4.815636
265.857172	8000.412438	10.322023	-0.054618	4.815651
265.365034	8000.391567	10.327027	-0.054527	4.815647
265.482609	8000.415922	10.332032	-0.054549	4.815654
265.601987	8000.403990	10.337037	-0.054571	4.815650
265.683985	8000.308135	10.342042	-0.054586	4.815621
265.655505	8000.421957	10.347047	-0.054581	4.815655
265.585870	8000.363140	10.352051	-0.054568	4.815638
265.734282	8000.454222	10.357056	-0.054595	4.815664
265.583619	8000.416509	10.362061	-0.054567	4.815653
265.639668	8000.391792	10.367066	-0.054578	4.815646
265.677720	8000.396688	10.372071	-0.054585	4.815647
265.640789	8000.372585	10.377075	-0.054578	4.815640
265.650560	8000.396244	10.382080	-0.054580	4.815647
265.659639	8000.423096	10.387085	-0.054582	4.815655
265.444345	8000.355486	10.392090	-0.054541	4.815636
265.595013	8000.438060	10.397095	-0.054570	4.815660
265.781482	8000.412273	10.402099	-0.054604	4.815651
265.872492	8000.421240	10.407104	-0.054621	4.815653
265.785200	8000.399518	10.412109	-0.054605	4.815647
265.800899	8000.368800	10.417114	-0.054608	4.815638
265.947604	8000.445969	10.422119	-0.054635	4.815660
265.782642	8000.406954	10.427123	-0.054604	4.815650
265.834784	8000.413148	10.432128	-0.054614	4.815651
265.693957	8000.417252	10.437133	-0.054588	4.815653
265.684075	8000.314553	10.442138	-0.054586	4.815623
265.809999	8000.371087	10.447143	-0.054610	4.815639
265.798820	8000.362360	10.452147	-0.054607	4.815636
265.712303	8000.426099	10.457152	-0.054591	4.815656
265.632214	8000.374588	10.462157	-0.054576	4.815641
265.776124	8000.329946	10.467162	-0.054603	4.815627
265.839194	8000.447403	10.472167	-0.054615	4.815661
265.570437	8000.452618	10.477171	-0.054565	4.815664
265.585143	8000.435769	10.482176	-0.054568	4.815659
265.672651	8000.412635	10.487181	-0.054584	4.815652
265.569113	8000.346855	10.492186	-0.054565	4.815633
265.728703	8000.395395	10.497191	-0.054594	4.815646
265.695384	8000.342513	10.502195	-0.054588	4.815631
265.943134	8000.360453	10.507200	-0.054634	4.815635
265.975786	8000.396236	10.512205	-0.054640	4.815646
265.856219	8000.269310	10.517210	-0.054618	4.815609
265.925980	8000.383672	10.522215	-0.054631	4.815642
265.742430	8000.438347	10.527219	-0.054597	4.815659
265.876950	8000.389279	10.532224	-0.054622	4.815644
265.880557	8000.370112	10.537229	-0.054623	4.815638
265.773029	8000.351263	10.542234	-0.054603	4.815633
265.793507	8000.369757	10.547239	-0.054607	4.815639
265.835440	8000.321310	10.552243	-0.054614	4.815624
265.996568	8000.394443	10.557248	-0.054644	4.815645
265.743884	8000.373218	10.562253	-0.054597	4.815640
265.822717	8000.358487	10.567258	-0.054612	4.815635
265.864684	8000.382673	10.572263	-0.054620	4.815642
265.960073	8000.360736	10.577267	-0.054638	4.815635
266.016886	8000.394778	10.582272	-0.054648	4.815645
265.782978	8000.435810	10.587277	-0.054605	4.815658
265.680367	8000.344410	10.592282	-0.054586	4.815632
265.841634	8000.370548	10.597287	-0.054616	4.815639
265.770827	8000.332006	10.602291	-0.054602	4.815628
265.838310	8000.408947	10.607296	-0.054615	4.815650
265.904871	8000.389742	10.612301	-0.054627	4.815644
265.906760	8000.374820	10.617306	-0.054628	4.815640
265.993093	8000.373029	10.622311	-0.054644	4.815639
265.647118	8000.336392	10.627315	-0.054579	4.815630
265.801200	8000.319688	10.632320	-0.054608	4.815624
265.919470	8000.332305	10.637325	-0.054630	4.815627
265.817946	8000.342393	10.642330	-0.054611	4.815631
266.052059	8000.439151	10.647335	-0.054655	4.815658
266.059187	8000.357023	10.652339	-0.054656	4.815634
266.066731	8000.403076	10.657344	-0.054658	4.815647
265.976314	8000.428299	10.662349	-0.054641	4.815655
265.756615	8000.391592	10.667354	-0.054600	4.815645
265.968169	8000.436712	10.672359	-0.054639	4.815657
266.058469	8000.409351	10.677363	-0.054656	4.815649
265.877044	8000.380747	10.682368	-0.054622	4.815641
265.870389	8000.411614	10.687373	-0.054621	4.815651
265.991171	8000.440294	10.692378	-0.054644	4.815658
266.022954	8000.432270	10.697383	-0.054649	4.815656
265.856319	8000.369728	10.702387	-0.054618	4.815638
265.934647	8000.424416	10.707392	-0.054633	4.815654
266.012249	8000.432096	10.712397	-0.054647	4.815656
266.078021	8000.413946	10.717402	-0.054660	4.815650
266.194671	8000.395562	10.722407	-0.054681	4.815644
266.113725	8000.386760	10.727411	-0.054666	4.815642
266.200403	8000.458676	10.732416	-0.054683	4.815663
266.130082	8000.438299	10.737421	-0.054669	4.815657
266.244221	8000.411328	10.742426	-0.054691	4.815649
266.154605	8000.432292	10.747431	-0.054674	4.815655
265.864096	8000.364519	10.752435	-0.054620	4.815637
266.024135	8000.449384	10.757440	-0.054650	4.815661
266.029049	8000.453737	10.762445	-0.054651	4.815662
266.104284	8000.291547	10.767450	-0.054665	4.815614
266.083308	8000.379857	10.772455	-0.054661	4.815640
266.100922	8000.280811	10.777459	-0.054664	4.815611
266.051713	8000.321663	10.782464	-0.054655	4.815623
266.092216	8000.412048	10.787469	-0.054662	4.815650
266.144695	8000.359501	10.792474	-0.054672	4.815634
266.198428	8000.405242	10.797479	-0.054682	4.815647
266.147927	8000.351010	10.802483	-0.054673	4.815631
266.255543	8000.383747	10.807488	-0.054693	4.815641
265.800268	8000.429702	10.812493	-0.054608	4.815656
265.815439	8000.355183	10.817498	-0.054611	4.815634
266.126226	8000.342111	10.822503	-0.054669	4.815629
266.045019	8000.348259	10.827507	-0.054654	4.815631
266.091667	8000.314844	10.832512	-0.054662	4.815621
266.227175	8000.380081	10.837517	-0.054688	4.815640
266.374120	8000.358988	10.842522	-0.054715	4.815633
266.334693	8000.426703	10.847527	-0.054708	4.815653
266.166202	8000.392969	10.852531	-0.054676	4.815644
265.979807	8000.414486	10.857536	-0.054642	4.815651
266.013342	8000.452419	10.862541	-0.054648	4.815662
266.051783	8000.376144	10.867546	-0.054655	4.815639
266.254939	8000.425399	10.872551	-0.054693	4.815653
266.149915	8000.387364	10.877555	-0.054673	4.815642
266.077162	8000.418217	10.882560	-0.054660	4.815651
265.885445	8000.440715	10.887565	-0.054624	4.815659
265.931146	8000.341060	10.892570	-0.054632	4.815630
266.199951	8000.391389	10.897575	-0.054683	4.815643
266.077540	8000.403271	10.902579	-0.054660	4.815647
266.080421	8000.367003	10.907584	-0.054660	4.815636
266.181978	8000.401777	10.912589	-0.054679	4.815646
265.958443	8000.338304	10.917594	-0.054638	4.815629
266.107978	8000.430474	10.922599	-0.054665	4.815655
265.995776	8000.332507	10.927603	-0.054645	4.815627
266.166227	8000.354524	10.932608	-0.054676	4.815632
266.081730	8000.394798	10.937613	-0.054661	4.815645
265.982702	8000.320545	10.942618	-0.054642	4.815623
266.029459	8000.458030	10.947623	-0.054651	4.815663
266.095167	8000.428131	10.952627	-0.054663	4.815654
266.028043	8000.430237	10.957632	-0.054651	4.815655
266.264532	8000.379634	10.962637	-0.054695	4.815639
265.997226	8000.329330	10.967642	-0.054645	4.815626
266.288123	8000.385361	10.972647	-0.054699	4.815641
266.344924	8000.325408	10.977651	-0.054710	4.815623
266.243489	8000.369678	10.982656	-0.054691	4.815636
266.283379	8000.366058	10.987661	-0.054698	4.815635
266.327026	8000.344343	10.992666	-0.054706	4.815629
266.266671	8000.455508	10.997671	-0.054695	4.815661
266.107592	8000.442223	11.002675	-0.054665	4.815658
266.146258	8000.406540	11.007680	-0.054673	4.815648
266.332670	8000.426682	11.012685	-0.054707	4.815653
266.120797	8000.332424	11.017690	-0.054668	4.815626
266.357593	8000.366208	11.022695	-0.054712	4.815635
266.356525	8000.342692	11.027699	-0.054712	4.815628
266.250873	8000.349508	11.032704	-0.054692	4.815631
266.105686	8000.424037	11.037709	-0.054665	4.815653
266.199956	8000.392468	11.042714	-0.054683	4.815643
266.306367	8000.455094	11.047719	-0.054703	4.815661
266.161056	8000.385424	11.052723	-0.054675	4.815641
266.114316	8000.334457	11.057728	-0.054667	4.815627
266.298090	8000.389804	11.062733	-0.054701	4.815642
266.184968	8000.307843	11.067738	-0.054680	4.815619
266.241174	8000.410235	11.072743	-0.054690	4.815648
266.340976	8000.377689	11.077747	-0.054709	4.815638
266.369676	8000.352524	11.082752	-0.054714	4.815631
266.496887	8000.430444	11.087757	-0.054738	4.815653
266.534295	8000.379787	11.092762	-0.054745	4.815638
266.688916	8000.463497	11.097767	-0.054774	4.815662
266.434974	8000.412342	11.102771	-0.054726	4.815648
266.204520	8000.394684	11.107776	-0.054684	4.815644
266.414214	8000.424820	11.112781	-0.054723	4.815652
266.255336	8000.383767	11.117786	-0.054693	4.815641
266.184062	8000.463779	11.122791	-0.054680	4.815664
266.316827	8000.422159	11.127795	-0.054705	4.815651
266.245735	8000.360113	11.132800	-0.054691	4.815634
266.192798	8000.417993	11.137805	-0.054681	4.815651
266.228735	8000.368380	11.142810	-0.054688	4.815636
266.142783	8000.405426	11.147815	-0.054672	4.815647
266.043571	8000.413416	11.152819	-0.054654	4.815650
266.143654	8000.427872	11.157824	-0.054672	4.815654
266.209063	8000.431079	11.162829	-0.054684	4.815655
266.261508	8000.388145	11.167834	-0.054694	4.815642
266.278494	8000.438625	11.172839	-0.054697	4.815656
266.172542	8000.396302	11.177843	-0.054678	4.815645
266.471888	8000.298663	11.182848	-0.054733	4.815615
266.325115	8000.437253	11.187853	-0.054706	4.815656
266.183845	8000.350559	11.192858	-0.054680	4.815631
266.362043	8000.315024	11.197863	-0.054713	4.815620
266.162403	8000.325642	11.202867	-0.054676	4.815624
266.117228	8000.321699	11.207872	-0.054667	4.815623
266.264330	8000.382854	11.212877	-0.054695	4.815640
266.269640	8000.363715	11.217882	-0.054696	4.815635
266.335771	8000.392569	11.222887	-0.054708	4.815643
266.318941	8000.366659	11.227891	-0.054705	4.815635
266.378444	8000.320636	11.232896	-0.054716	4.815621
266.272953	8000.386201	11.237901	-0.054696	4.815641
266.285650	8000.292415	11.242906	-0.054699	4.815614
266.471550	8000.369158	11.247911	-0.054733	4.815635
266.308006	8000.396389	11.252915	-0.054703	4.815644
266.437122	8000.349369	11.257920	-0.054727	4.815630
266.344519	8000.362808	11.262925	-0.054710	4.815634
266.388480	8000.318666	11.267930	-0.054718	4.815621
266.284474	8000.363962	11.272935	-0.054699	4.815635
266.163706	8000.363054	11.277939	-0.054676	4.815635
266.368123	8000.343969	11.282944	-0.054714	4.815628
266.359402	8000.336350	11.287949	-0.054713	4.815626
266.298793	8000.355653	11.292954	-0.054701	4.815632
266.481396	8000.408844	11.297959	-0.054735	4.815647
266.544264	8000.389579	11.302963	-0.054747	4.815641
266.541269	8000.317966	11.307968	-0.054746	4.815620
266.554374	8000.384405	11.312973	-0.054749	4.815639
266.599922	8000.358448	11.317978	-0.054757	4.815631
266.466801	8000.391517	11.322983	-0.054733	4.815642
266.397030	8000.416010	11.327987	-0.054720	4.815649
266.530192	8000.373329	11.332992	-0.054744	4.815636
266.523174	8000.425553	11.337997	-0.054743	4.815651
266.425459	8000.320345	11.343002	-0.054725	4.815621
266.588335	8000.425552	11.348007	-0.054755	4.815651
266.674208	8000.435504	11.353011	-0.054771	4.815654
266.539907	8000.431169	11.358016	-0.054746	4.815653
266.676744	8000.453705	11.363021	-0.054772	4.815659
266.477205	8000.308377	11.368026	-0.054735	4.815617
266.653435	8000.453324	11.373031	-0.054767	4.815659
266.532610	8000.378713	11.378035	-0.054745	4.815638
266.531311	8000.384033	11.383040	-0.054745	4.815639
266.536868	8000.421509	11.388045	-0.054746	4.815650
266.491531	8000.291523	11.393050	-0.054737	4.815612
266.544358	8000.408814	11.398055	-0.054747	4.815646
266.628805	8000.384562	11.403059	-0.054763	4.815639
266.419967	8000.358713	11.408064	-0.054724	4.815632
266.444786	8000.409322	11.413069	-0.054729	4.815647
266.548371	8000.321295	11.418074	-0.054748	4.815621
266.701569	8000.399641	11.423079	-0.054776	4.815643
266.551472	8000.335232	11.428083	-0.054748	4.815625
266.640724	8000.390100	11.433088	-0.054765	4.815641
266.696047	8000.393142	11.438093	-0.054775	4.815641
266.585099	8000.371032	11.443098	-0.054755	4.815635
266.631605	8000.438018	11.448103	-0.054763	4.815655
266.767940	8000.401798	11.453107	-0.054789	4.815643
266.601788	8000.388396	11.458112	-0.054758	4.815640
266.487502	8000.421774	11.463117	-0.054737	4.815651
266.656833	8000.329483	11.468122	-0.054768	4.815623
266.650265	8000.403077	11.473127	-0.054767	4.815644
266.592332	8000.383971	11.478131	-0.054756	4.815639
266.508651	8000.325990	11.483136	-0.054740	4.815622
266.734601	8000.329689	11.488141	-0.054783	4.815622
266.550223	8000.298900	11.493146	-0.054748	4.815614
266.650658	8000.310158	11.498151	-0.054767	4.815617
266.592560	8000.315616	11.503155	-0.054756	4.815619
266.714835	8000.306937	11.508160	-0.054779	4.815616
266.724602	8000.361572	11.513165	-0.054781	4.815632
266.707262	8000.316427	11.518170	-0.054777	4.815619
266.716734	8000.343285	11.523175	-0.054779	4.815626
266.720251	8000.402091	11.528179	-0.054780	4.815644
266.691665	8000.306559	11.533184	-0.054775	4.815616
266.603194	8000.344632	11.538189	-0.054758	4.815627
266.519607	8000.312289	11.543194	-0.054743	4.815618
266.684676	8000.419668	11.548199	-0.054773	4.815649
266.865864	8000.420499	11.553203	-0.054807	4.815648
266.572092	8000.334511	11.558208	-0.054752	4.815625
266.522733	8000.440517	11.563213	-0.054743	4.815656
266.674733	8000.359691	11.568218	-0.054772	4.815631
266.833579	8000.403950	11.573223	-0.054801	4.815644
266.606081	8000.357500	11.578227	-0.054759	4.815631
266.684637	8000.347037	11.583232	-0.054773	4.815628
266.640619	8000.386906	11.588237	-0.054765	4.815640
266.602052	8000.365980	11.593242	-0.054758	4.815634
266.739769	8000.421642	11.598247	-0.054784	4.815649
266.687090	8000.405826	11.603251	-0.054774	4.815645
266.529062	8000.354105	11.608256	-0.054744	4.815631
266.503201	8000.423111	11.613261	-0.054740	4.815651
266.758833	8000.397388	11.618266	-0.054787	4.815642
266.763997	8000.375043	11.623271	-0.054788	4.815636
266.580075	8000.348533	11.628275	-0.054754	4.815629
266.568069	8000.336587	11.633280	-0.054752	4.815625
266.538388	8000.426893	11.638285	-0.054746	4.815652
266.453943	8000.377445	11.643290	-0.054730	4.815638
266.559897	8000.413360	11.648295	-0.054750	4.815648
266.621908	8000.436807	11.653299	-0.054762	4.815654
266.607177	8000.394909	11.658304	-0.054759	4.815642
266.611555	8000.432365	11.663309	-0.054760	4.815653
266.485817	8000.361947	11.668314	-0.054736	4.815633
266.775838	8000.428647	11.673319	-0.054790	4.815651
266.655358	8000.427743	11.678323	-0.054768	4.815651
266.697519	8000.396390	11.683328	-0.054776	4.815642
266.680745	8000.384366	11.688333	-0.054773	4.815639
266.881385	8000.313950	11.693338	-0.054810	4.815617
266.731240	8000.412965	11.698343	-0.054782	4.815647
266.743832	8000.386468	11.703347	-0.054785	4.815639
266.724894	8000.288958	11.708352	-0.054781	4.815611
266.667231	8000.349966	11.713357	-0.054770	4.815629
266.590788	8000.289968	11.718362	-0.054756	4.815611
266.668996	8000.378835	11.723367	-0.054771	4.815637
266.501508	8000.335505	11.728371	-0.054739	4.815625
266.627401	8000.325817	11.733376	-0.054763	4.815622
266.707761	8000.383744	11.738381	-0.054778	4.815638
266.594669	8000.353053	11.743386	-0.054757	4.815630
266.714777	8000.387064	11.748391	-0.054779	4.815639
266.706625	8000.336728	11.753395	-0.054778	4.815625
266.507304	8000.293945	11.758400	-0.054740	4.815613
266.591990	8000.380782	11.763405	-0.054756	4.815638
266.706002	8000.330311	11.768410	-0.054777	4.815623
266.686140	8000.406891	11.773415	-0.054774	4.815645
266.571483	8000.351608	11.778419	-0.054752	4.815630
266.589311	8000.326265	11.783424	-0.054756	4.815622
266.710718	8000.378455	11.788429	-0.054778	4.815637
266.644720	8000.365626	11.793434	-0.054766	4.815633
266.568127	8000.370781	11.798439	-0.054752	4.815635
266.661690	8000.413970	11.803443	-0.054769	4.815647
266.681397	8000.338456	11.808448	-0.054773	4.815625
266.568301	8000.398556	11.813453	-0.054752	4.815643
266.539891	8000.320118	11.818458	-0.054747	4.815621
266.731588	8000.342483	11.823463	-0.054782	4.815626
266.706416	8000.371979	11.828467	-0.054778	4.815635
266.663306	8000.331753	11.833472	-0.054770	4.815623
266.715684	8000.420198	11.838477	-0.054779	4.815649
266.532766	8000.361661	11.843482	-0.054745	4.815633
266.634087	8000.403909	11.848487	-0.054764	4.815645
266.589293	8000.343360	11.853491	-0.054756	4.815627
266.611871	8000.330913	11.858496	-0.054760	4.815623
266.573278	8000.392233	11.863501	-0.054753	4.815641
266.402867	8000.360604	11.868506	-0.054721	4.815633
266.696544	8000.363276	11.873511	-0.054776	4.815632
266.711053	8000.373127	11.878515	-0.054779	4.815635
266.566651	8000.320561	11.883520	-0.054752	4.815621
266.665293	8000.372379	11.888525	-0.054770	4.815635
266.593176	8000.378675	11.893530	-0.054757	4.815637
266.737176	8000.442985	11.898535	-0.054783	4.815656
266.416750	8000.382197	11.903539	-0.054724	4.815639
266.616163	8000.355554	11.908544	-0.054761	4.815631
266.532931	8000.326420	11.913549	-0.054745	4.815622
266.547200	8000.314905	11.918554	-0.054748	4.815619
266.640352	8000.370905	11.923559	-0.054765	4.815635
266.678659	8000.385418	11.928563	-0.054773	4.815639
266.692359	8000.341849	11.933568	-0.054775	4.815626
266.595819	8000.379790	11.938573	-0.054757	4.815638
266.631296	8000.371826	11.943578	-0.054764	4.815635
266.626838	8000.366413	11.948583	-0.054763	4.815634
266.679650	8000.360869	11.953587	-0.054773	4.815632
266.920443	8000.338108	11.958592	-0.054818	4.815624
266.784818	8000.382886	11.963597	-0.054792	4.815638
266.588520	8000.321994	11.968602	-0.054756	4.815621
266.974897	8000.381727	11.973607	-0.054828	4.815636
266.703261	8000.370871	11.978611	-0.054777	4.815635
266.662472	8000.281549	11.983616	-0.054770	4.815609
266.631439	8000.368628	11.988621	-0.054764	4.815634
266.951586	8000.308713	11.993626	-0.054823	4.815615
266.865888	8000.385284	11.998631	-0.054807	4.815638
266.714309	8000.377462	12.003635	-0.054779	4.815636
266.779580	8000.435143	12.008640	-0.054791	4.815653
266.876713	8000.461301	12.013645	-0.054810	4.815660
266.773249	8000.351725	12.018650	-0.054790	4.815629
266.774675	8000.394474	12.023655	-0.054791	4.815641
266.812001	8000.382268	12.028659	-0.054797	4.815637
266.603896	8000.341477	12.033664	-0.054759	4.815626
266.873981	8000.445236	12.038669	-0.054809	4.815656
266.645312	8000.389153	12.043674	-0.054766	4.815640
266.618613	8000.390853	12.048679	-0.054761	4.815641
266.573250	8000.358067	12.053683	-0.054753	4.815631
266.776989	8000.278088	12.058688	-0.054791	4.815607
266.683919	8000.350266	12.063693	-0.054774	4.815629
266.624028	8000.306561	12.068698	-0.054762	4.815616
266.694288	8000.346164	12.073703	-0.054776	4.815627
266.875307	8000.387581	12.078707	-0.054809	4.815639
266.735105	8000.355378	12.083712	-0.054783	4.815630
266.730643	8000.380941	12.088717	-0.054782	4.815637
266.773279	8000.356004	12.093722	-0.054790	4.815630
266.699254	8000.406063	12.098727	-0.054777	4.815645
266.774584	8000.434000	12.103731	-0.054791	4.815653
266.738844	8000.399235	12.108736	-0.054784	4.815643
266.944065	8000.434639	12.113741	-0.054822	4.815652
266.762411	8000.321647	12.118746	-0.054788	4.815620
266.725934	8000.340277	12.123751	-0.054782	4.815626
266.789734	8000.413955	12.128755	-0.054793	4.815647
266.752821	8000.324696	12.133760	-0.054787	4.815621
266.761664	8000.411360	12.138765	-0.054788	4.815646
266.755918	8000.317271	12.143770	-0.054787	4.815619
266.950163	8000.315110	12.148775	-0.054823	4.815617
266.711615	8000.357135	12.153779	-0.054779	4.815631
266.783887	8000.352978	12.158784	-0.054792	4.815629
267.008595	8000.374816	12.163789	-0.054834	4.815634
266.825314	8000.382497	12.168794	-0.054800	4.815637
266.653290	8000.429883	12.173799	-0.054768	4.815652
266.656785	8000.412850	12.178803	-0.054769	4.815647
266.797943	8000.323302	12.183808	-0.054795	4.815620
266.794979	8000.385206	12.188813	-0.054794	4.815638
266.767857	8000.358059	12.193818	-0.054789	4.815631
267.091937	8000.364433	12.198823	-0.054850	4.815631
266.964350	8000.373026	12.203827	-0.054826	4.815634
266.835435	8000.334599	12.208832	-0.054802	4.815623
266.974906	8000.420198	12.213837	-0.054828	4.815648
266.727911	8000.420427	12.218842	-0.054782	4.815649
266.773302	8000.409421	12.223847	-0.054790	4.815646
266.910823	8000.445853	12.228851	-0.054816	4.815656
266.909992	8000.414864	12.233856	-0.054816	4.815646
266.898382	8000.461673	12.238861	-0.054814	4.815660
266.888564	8000.310905	12.243866	-0.054812	4.815616
266.904686	8000.338940	12.248871	-0.054815	4.815624
266.681343	8000.415394	12.253875	-0.054773	4.815648
266.694481	8000.375021	12.258880	-0.054776	4.815636
266.944511	8000.430386	12.263885	-0.054822	4.815651
266.885953	8000.425155	12.268890	-0.054811	4.815650
266.862509	8000.417294	12.273895	-0.054807	4.815647
266.935482	8000.325561	12.278899	-0.054821	4.815620
266.850558	8000.308149	12.283904	-0.054805	4.815616
266.957160	8000.353688	12.288909	-0.054825	4.815628
266.993700	8000.386331	12.293914	-0.054832	4.815638
267.082626	8000.399537	12.298919	-0.054848	4.815641
266.811844	8000.436761	12.303923	-0.054798	4.815653
266.693879	8000.405991	12.308928	-0.054776	4.815645
266.995935	8000.432300	12.313933	-0.054832	4.815651
266.892311	8000.353697	12.318938	-0.054813	4.815629
266.924435	8000.398017	12.323943	-0.054819	4.815641
266.975080	8000.435164	12.328947	-0.054828	4.815652
267.012949	8000.387718	12.333952	-0.054835	4.815638
267.080701	8000.440098	12.338957	-0.054848	4.815653
266.970688	8000.352846	12.343962	-0.054827	4.815628
267.097679	8000.411537	12.348967	-0.054851	4.815645
266.873695	8000.431369	12.353971	-0.054809	4.815651
266.820099	8000.355722	12.358976	-0.054799	4.815630
266.995284	8000.417339	12.363981	-0.054832	4.815647
266.841167	8000.311206	12.368986	-0.054803	4.815616
266.708996	8000.327201	12.373991	-0.054779	4.815622
266.637759	8000.381578	12.378995	-0.054765	4.815638
266.823587	8000.291693	12.384000	-0.054800	4.815611
266.752555	8000.347142	12.389005	-0.054787	4.815627
266.721508	8000.356247	12.394010	-0.054781	4.815630
266.956897	8000.372919	12.399015	-0.054825	4.815634
266.806171	8000.405700	12.404019	-0.054797	4.815644
266.697318	8000.376147	12.409024	-0.054776	4.815636
266.978193	8000.421335	12.414029	-0.054829	4.815648
267.012992	8000.367430	12.419034	-0.054835	4.815632
266.993381	8000.364973	12.424039	-0.054832	4.815631
266.884799	8000.393104	12.429043	-0.054811	4.815640
266.858249	8000.404419	12.434048	-0.054806	4.815644
266.972482	8000.440470	12.439053	-0.054828	4.815654
267.011694	8000.331094	12.444058	-0.054835	4.815621
267.076448	8000.364199	12.449063	-0.054847	4.815631
266.959277	8000.443459	12.454067	-0.054825	4.815655
266.727617	8000.388396	12.459072	-0.054782	4.815640
266.963324	8000.381574	12.464077	-0.054826	4.815636
266.888453	8000.381417	12.469082	-0.054812	4.815637
266.906053	8000.383842	12.474087	-0.054815	4.815637
266.856596	8000.420417	12.479091	-0.054806	4.815648
266.940204	8000.336335	12.484096	-0.054822	4.815623
267.040122	8000.360403	12.489101	-0.054840	4.815630
267.020713	8000.397470	12.494106	-0.054837	4.815641
267.151573	8000.376114	12.499111	-0.054861	4.815634
267.167934	8000.432994	12.504115	-0.054864	4.815651
267.070152	8000.339533	12.509120	-0.054846	4.815624
267.048442	8000.412880	12.514125	-0.054842	4.815645
267.226182	8000.373065	12.519130	-0.054875	4.815633
267.145765	8000.393111	12.524135	-0.054860	4.815639
267.070913	8000.477338	12.529139	-0.054846	4.815664
267.143383	8000.386664	12.534144	-0.054860	4.815637
267.374106	8000.471622	12.539149	-0.054903	4.815661
267.134393	8000.397199	12.544154	-0.054858	4.815640
267.193578	8000.412055	12.549159	-0.054869	4.815644
267.130507	8000.423840	12.554163	-0.054857	4.815648
267.078449	8000.387739	12.559168	-0.054848	4.815638
266.991056	8000.462147	12.564173	-0.054831	4.815660
266.990991	8000.436511	12.569178	-0.054831	4.815652
266.965751	8000.328215	12.574183	-0.054827	4.815621
266.972828	8000.447963	12.579187	-0.054828	4.815656
266.919412	8000.373387	12.584192	-0.054818	4.815634
267.167499	8000.467174	12.589197	-0.054864	4.815660
266.962916	8000.460620	12.594202	-0.054826	4.815660
267.109617	8000.411752	12.599207	-0.054853	4.815645
267.224164	8000.432855	12.604211	-0.054875	4.815650
267.128069	8000.328739	12.609216	-0.054857	4.815620
267.082875	8000.345090	12.614221	-0.054848	4.815625
267.177625	8000.378686	12.619226	-0.054866	4.815635
267.102671	8000.394549	12.624231	-0.054852	4.815640
267.135181	8000.373719	12.629235	-0.054858	4.815633
267.155295	8000.338800	12.634240	-0.054862	4.815623
267.303846	8000.397845	12.639245	-0.054890	4.815640
267.112578	8000.322079	12.644250	-0.054854	4.815618
266.962604	8000.364486	12.649255	-0.054826	4.815631
267.108228	8000.458732	12.654259	-0.054853	4.815658
267.121910	8000.435457	12.659264	-0.054856	4.815651
267.211233	8000.492464	12.664269	-0.054872	4.815668
267.416993	8000.396496	12.669274	-0.054911	4.815639
267.260758	8000.341598	12.674279	-0.054882	4.815623
267.246259	8000.412927	12.679283	-0.054879	4.815644
267.138556	8000.317167	12.684288	-0.054859	4.815617
267.520494	8000.394988	12.689293	-0.054930	4.815638
267.113641	8000.341327	12.694298	-0.054854	4.815624
267.135339	8000.363046	12.699303	-0.054858	4.815630
267.345579	8000.394261	12.704307	-0.054897	4.815638
267.195725	8000.320241	12.709312	-0.054869	4.815617
267.111879	8000.361595	12.714317	-0.054854	4.815630
267.099600	8000.315464	12.719322	-0.054852	4.815616
267.147011	8000.348285	12.724327	-0.054860	4.815626
267.168002	8000.414854	12.729331	-0.054864	4.815645
267.019805	8000.286387	12.734336	-0.054837	4.815608
267.157223	8000.434973	12.739341	-0.054862	4.815651
267.030025	8000.392301	12.744346	-0.054839	4.815639
267.234550	8000.349720	12.749351	-0.054877	4.815626
267.374261	8000.322100	12.754355	-0.054903	4.815617
267.231199	8000.283441	12.759360	-0.054876	4.815606
267.272971	8000.437939	12.764365	-0.054884	4.815651
267.362912	8000.445821	12.769370	-0.054901	4.815653
267.242278	8000.346644	12.774375	-0.054878	4.815625
267.253123	8000.392752	12.779379	-0.054880	4.815638
267.137946	8000.358822	12.784384	-0.054859	4.815629
267.315769	8000.355326	12.789389	-0.054892	4.815627
267.228275	8000.323985	12.794394	-0.054876	4.815618
267.151154	8000.315246	12.799399	-0.054861	4.815616
267.059794	8000.370362	12.804403	-0.054844	4.815633
267.076619	8000.362093	12.809408	-0.054847	4.815630
267.055508	8000.391655	12.814413	-0.054844	4.815639
267.069923	8000.353439	12.819418	-0.054846	4.815628
267.099588	8000.299450	12.824423	-0.054852	4.815612
267.248879	8000.348893	12.829427	-0.054879	4.815626
267.284607	8000.329183	12.834432	-0.054886	4.815620
267.483523	8000.339918	12.839437	-0.054923	4.815622
267.342721	8000.329067	12.844442	-0.054897	4.815619
267.215490	8000.393210	12.849447	-0.054873	4.815639
267.284773	8000.442411	12.854451	-0.054886	4.815653
267.336395	8000.402667	12.859456	-0.054896	4.815641
267.335511	8000.416539	12.864461	-0.054896	4.815645
267.206932	8000.311892	12.869466	-0.054872	4.815615
267.271738	8000.285182	12.874471	-0.054884	4.815607
267.102656	8000.420204	12.879475	-0.054852	4.815647
267.227195	8000.333588	12.884480	-0.054875	4.815621
267.257152	8000.390690	12.889485	-0.054881	4.815638
267.195077	8000.469786	12.894490	-0.054870	4.815661
267.317740	8000.342548	12.899495	-0.054892	4.815623
267.407673	8000.389952	12.904499	-0.054909	4.815637
267.340500	8000.383512	12.909504	-0.054897	4.815635
267.320994	8000.425919	12.914509	-0.054893	4.815648
267.091438	8000.361275	12.919514	-0.054850	4.815630
267.308994	8000.338135	12.924519	-0.054891	4.815622
267.568316	8000.395789	12.929523	-0.054939	4.815638
267.286329	8000.393308	12.934528	-0.054887	4.815638
267.265322	8000.415395	12.939533	-0.054883	4.815645
267.464616	8000.407978	12.944538	-0.054920	4.815642
267.152068	8000.416746	12.949543	-0.054862	4.815646
267.147999	8000.442315	12.954547	-0.054861	4.815653
267.127209	8000.342638	12.959552	-0.054857	4.815624
267.245106	8000.409726	12.964557	-0.054879	4.815643
267.217160	8000.370815	12.969562	-0.054874	4.815632
267.364285	8000.403133	12.974567	-0.054901	4.815641
267.228753	8000.443640	12.979571	-0.054876	4.815653
267.024854	8000.279012	12.984576	-0.054838	4.815606
267.129683	8000.397156	12.989581	-0.054857	4.815640
267.266908	8000.368427	12.994586	-0.054883	4.815631
267.085891	8000.357986	12.999591	-0.054849	4.815629
267.277498	8000.368601	13.004595	-0.054885	4.815631
267.407444	8000.353639	13.009600	-0.054909	4.815626
267.303940	8000.435260	13.014605	-0.054890	4.815651
267.347280	8000.403926	13.019610	-0.054898	4.815641
267.299998	8000.350813	13.024615	-0.054889	4.815626
267.394860	8000.404706	13.029619	-0.054907	4.815641
267.257580	8000.345846	13.034624	-0.054881	4.815625
267.228557	8000.405188	13.039629	-0.054876	4.815642
267.233736	8000.356138	13.044634	-0.054877	4.815628
267.190679	8000.405636	13.049639	-0.054869	4.815642
267.233458	8000.452268	13.054643	-0.054877	4.815656
267.221754	8000.398669	13.059648	-0.054875	4.815640
267.364871	8000.468307	13.064653	-0.054901	4.815660
267.228732	8000.420147	13.069658	-0.054876	4.815646
267.234948	8000.411704	13.074663	-0.054877	4.815644
267.252379	8000.424807	13.079667	-0.054880	4.815648
267.194442	8000.354429	13.084672	-0.054870	4.815627
267.356244	8000.384851	13.089677	-0.054900	4.815636
267.352119	8000.426442	13.094682	-0.054899	4.815648
267.216613	8000.347317	13.099687	-0.054874	4.815625
267.257940	8000.456945	13.104691	-0.054881	4.815657
267.472039	8000.381408	13.109696	-0.054921	4.815634
267.572641	8000.426851	13.114701	-0.054940	4.815647
267.378462	8000.411921	13.119706	-0.054904	4.815643
267.427288	8000.377472	13.124711	-0.054913	4.815633
267.499494	8000.452358	13.129715	-0.054926	4.815655
267.377745	8000.417251	13.134720	-0.054904	4.815645
267.396049	8000.458141	13.139725	-0.054907	4.815657
267.416451	8000.393318	13.144730	-0.054911	4.815638
267.332419	8000.428260	13.149735	-0.054895	4.815648
267.301802	8000.456599	13.154739	-0.054890	4.815657
267.341695	8000.399572	13.159744	-0.054897	4.815640
267.399035	8000.410125	13.164749	-0.054908	4.815643
267.444605	8000.392713	13.169754	-0.054916	4.815637
267.522862	8000.348065	13.174759	-0.054931	4.815624
267.544470	8000.462712	13.179763	-0.054935	4.815657
267.122184	8000.379958	13.184768	-0.054856	4.815635
267.419038	8000.373069	13.189773	-0.054912	4.815632
267.489207	8000.393446	13.194778	-0.054925	4.815637
267.364034	8000.326239	13.199783	-0.054901	4.815618
267.273411	8000.357868	13.204787	-0.054884	4.815628
267.135933	8000.333186	13.209792	-0.054859	4.815621
267.361308	8000.374262	13.214797	-0.054901	4.815632
267.237916	8000.426718	13.219802	-0.054878	4.815648
267.245950	8000.377715	13.224807	-0.054879	4.815634
267.211205	8000.387828	13.229811	-0.054873	4.815637
267.323529	8000.340532	13.234816	-0.054894	4.815623
267.205074	8000.397341	13.239821	-0.054872	4.815640
267.482082	8000.446741	13.244826	-0.054923	4.815653
267.436521	8000.328498	13.249831	-0.054915	4.815619
267.468365	8000.437971	13.254835	-0.054921	4.815651
267.216867	8000.377241	13.259840	-0.054874	4.815634
267.281741	8000.443461	13.264845	-0.054886	4.815653
267.098972	8000.402015	13.269850	-0.054852	4.815642
267.252470	8000.335099	13.274855	-0.054881	4.815621
267.407839	8000.451936	13.279859	-0.054910	4.815655
267.076444	8000.321536	13.284864	-0.054848	4.815618
267.371790	8000.371235	13.289869	-0.054903	4.815631
267.302839	8000.318835	13.294874	-0.054890	4.815616
267.218579	8000.344160	13.299879	-0.054874	4.815624
267.273520	8000.388854	13.304883	-0.054885	4.815637
267.195000	8000.360865	13.309888	-0.054870	4.815629
267.387767	8000.421702	13.314893	-0.054906	4.815646
267.275240	8000.416655	13.319898	-0.054885	4.815645
267.296428	8000.359322	13.324903	-0.054889	4.815628
267.308055	8000.406511	13.329907	-0.054891	4.815642
267.325479	8000.399320	13.334912	-0.054894	4.815640
267.197784	8000.394025	13.339917	-0.054870	4.815639
267.144978	8000.399570	13.344922	-0.054861	4.815641
267.299022	8000.348685	13.349927	-0.054889	4.815625
267.356201	8000.382734	13.354931	-0.054900	4.815635
267.337616	8000.401657	13.359936	-0.054897	4.815641
267.447455	8000.428024	13.364941	-0.054917	4.815648
267.555928	8000.440482	13.369946	-0.054937	4.815651
267.391871	8000.374775	13.374951	-0.054907	4.815632
267.607073	8000.417821	13.379955	-0.054947	4.815644
267.378756	8000.358539	13.384960	-0.054904	4.815628
267.308196	8000.421472	13.389965	-0.054891	4.815646
267.298697	8000.419181	13.394970	-0.054889	4.815646
267.224892	8000.398746	13.399975	-0.054876	4.815640
267.342987	8000.454088	13.404979	-0.054898	4.815656
267.214651	8000.347308	13.409984	-0.054874	4.815625
267.547901	8000.451036	13.414989	-0.054936	4.815654
267.457671	8000.437809	13.419994	-0.054919	4.815651
267.426496	8000.386027	13.424999	-0.054913	4.815636
267.482542	8000.474534	13.430003	-0.054924	4.815661
267.340262	8000.407047	13.435008	-0.054897	4.815642
267.330961	8000.370578	13.440013	-0.054895	4.815631
267.254791	8000.374672	13.445018	-0.054881	4.815633
267.387938	8000.336263	13.450023	-0.054906	4.815621
267.458796	8000.369468	13.455027	-0.054919	4.815631
267.263759	8000.367343	13.460032	-0.054883	4.815631
267.425760	8000.400972	13.465037	-0.054913	4.815640
267.427717	8000.411686	13.470042	-0.054913	4.815643
267.392934	8000.357709	13.475047	-0.054907	4.815627
267.413936	8000.436029	13.480051	-0.054911	4.815650
267.446520	8000.408791	13.485056	-0.054917	4.815642
267.393441	8000.410058	13.490061	-0.054907	4.815643
267.377340	8000.437567	13.495066	-0.054904	4.815651
267.323561	8000.354439	13.500071	-0.054894	4.815627
267.409647	8000.453051	13.505075	-0.054910	4.815655
267.507297	8000.414061	13.510080	-0.054928	4.815643
267.576953	8000.438702	13.515085	-0.054941	4.815650
267.663994	8000.481786	13.520090	-0.054957	4.815662
267.522811	8000.437815	13.525095	-0.054931	4.815650
267.670171	8000.507524	13.530099	-0.054959	4.815670
267.544755	8000.457403	13.535104	-0.054935	4.815656
267.489890	8000.482140	13.540109	-0.054925	4.815663
267.410794	8000.469095	13.545114	-0.054910	4.815660
267.654214	8000.384425	13.550119	-0.054956	4.815634
267.592228	8000.467795	13.555123	-0.054944	4.815659
267.372948	8000.446045	13.560128	-0.054903	4.815653
267.538246	8000.443412	13.565133	-0.054934	4.815652
267.386341	8000.453742	13.570138	-0.054906	4.815656
267.586836	8000.380119	13.575143	-0.054943	4.815633
267.788611	8000.457128	13.580147	-0.054981	4.815655
267.662064	8000.385625	13.585152	-0.054957	4.815634
267.582489	8000.427048	13.590157	-0.054942	4.815647
267.695258	8000.447054	13.595162	-0.054963	4.815652
267.697626	8000.444957	13.600167	-0.054964	4.815651
267.495345	8000.469416	13.605171	-0.054926	4.815660
267.263539	8000.396190	13.610176	-0.054883	4.815639
267.370137	8000.405414	13.615181	-0.054903	4.815641
267.420809	8000.450038	13.620186	-0.054912	4.815654
267.388369	8000.407849	13.625191	-0.054906	4.815642
267.308325	8000.455674	13.630195	-0.054891	4.815656
267.280672	8000.385791	13.635200	-0.054886	4.815636
267.335887	8000.442240	13.640205	-0.054896	4.815652
267.414091	8000.382636	13.645210	-0.054911	4.815635
267.455683	8000.341660	13.650215	-0.054919	4.815622
267.755296	8000.452315	13.655219	-0.054975	4.815653
267.396387	8000.428278	13.660224	-0.054908	4.815648
267.404178	8000.426270	13.665229	-0.054909	4.815647
267.538672	8000.437018	13.670234	-0.054934	4.815650
267.620072	8000.414852	13.675239	-0.054949	4.815643
267.496393	8000.482257	13.680243	-0.054926	4.815663
267.547917	8000.395513	13.685248	-0.054936	4.815638
267.500773	8000.444944	13.690253	-0.054927	4.815652
267.584719	8000.474092	13.695258	-0.054943	4.815660
267.670161	8000.427424	13.700263	-0.054959	4.815646
267.512036	8000.448334	13.705267	-0.054929	4.815653
267.394056	8000.429312	13.710272	-0.054907	4.815648
267.488903	8000.450092	13.715277	-0.054925	4.815654
267.614785	8000.451087	13.720282	-0.054948	4.815654
267.632841	8000.383020	13.725287	-0.054952	4.815634
267.617605	8000.447929	13.730291	-0.054949	4.815653
267.604592	8000.379354	13.735296	-0.054947	4.815633
267.687542	8000.453348	13.740301	-0.054962	4.815654
267.669110	8000.465864	13.745306	-0.054959	4.815658
267.550594	8000.367789	13.750311	-0.054936	4.815630
267.583658	8000.428148	13.755315	-0.054943	4.815647
267.597833	8000.405949	13.760320	-0.054945	4.815641
267.714775	8000.446319	13.765325	-0.054967	4.815652
267.715766	8000.440995	13.770330	-0.054967	4.815650
267.622011	8000.424505	13.775335	-0.054950	4.815646
267.606027	8000.471243	13.780339	-0.054947	4.815660
267.653359	8000.384429	13.785344	-0.054956	4.815634
267.675024	8000.400807	13.790349	-0.054960	4.815639
267.405484	8000.419892	13.795354	-0.054910	4.815646
267.537818	8000.344084	13.800359	-0.054934	4.815623
267.725649	8000.452909	13.805363	-0.054969	4.815654
267.350165	8000.374125	13.810368	-0.054899	4.815632
267.592242	8000.441111	13.815373	-0.054944	4.815651
267.743513	8000.463884	13.820378	-0.054973	4.815657
267.438981	8000.420443	13.825383	-0.054916	4.815646
267.334597	8000.446506	13.830387	-0.054896	4.815654
267.425593	8000.452269	13.835392	-0.054913	4.815655
267.757944	8000.468395	13.840397	-0.054975	4.815658
267.549424	8000.471389	13.845402	-0.054936	4.815660
267.386853	8000.377933	13.850407	-0.054906	4.815633
267.589047	8000.417562	13.855411	-0.054944	4.815644
267.508854	8000.388477	13.860416	-0.054929	4.815636
267.570674	8000.414058	13.865421	-0.054940	4.815643
267.709251	8000.433418	13.870426	-0.054966	4.815648
267.578139	8000.386409	13.875431	-0.054942	4.815635
267.564512	8000.425708	13.880435	-0.054939	4.815646
267.540373	8000.399677	13.885440	-0.054935	4.815639
267.800585	8000.479779	13.890445	-0.054983	4.815661
267.453196	8000.487975	13.895450	-0.054919	4.815665
267.577319	8000.422714	13.900455	-0.054942	4.815646
267.717390	8000.494440	13.905459	-0.054968	4.815666
267.531743	8000.436923	13.910464	-0.054933	4.815650
267.717321	8000.508326	13.915469	-0.054968	4.815670
267.709143	8000.472942	13.920474	-0.054966	4.815660
267.671250	8000.431732	13.925479	-0.054959	4.815648
267.501247	8000.470606	13.930483	-0.054928	4.815660
267.419314	8000.444697	13.935488	-0.054912	4.815653
267.687426	8000.393544	13.940493	-0.054962	4.815636
267.645608	8000.448404	13.945498	-0.054954	4.815653
267.328191	8000.426115	13.950503	-0.054895	4.815648
267.560658	8000.432059	13.955507	-0.054939	4.815648
267.434044	8000.417168	13.960512	-0.054915	4.815645
267.570506	8000.396972	13.965517	-0.054940	4.815638
267.597503	8000.431596	13.970522	-0.054945	4.815648
267.529873	8000.405921	13.975527	-0.054933	4.815641
267.535591	8000.449809	13.980531	-0.054934	4.815654
267.574620	8000.385291	13.985536	-0.054941	4.815635
267.957643	8000.340293	13.990541	-0.055012	4.815620
267.746511	8000.415879	13.995546	-0.054973	4.815643
267.562350	8000.397909	14.000551	-0.054939	4.815638
267.884757	8000.455530	14.005555	-0.054999	4.815654
267.798008	8000.428474	14.010560	-0.054983	4.815646
267.609626	8000.478797	14.015565	-0.054948	4.815662
267.505511	8000.442911	14.020570	-0.054928	4.815652
267.525876	8000.373814	14.025575	-0.054932	4.815631
267.745005	8000.455379	14.030579	-0.054973	4.815654
267.483260	8000.417980	14.035584	-0.054924	4.815645
267.680338	8000.414799	14.040589	-0.054961	4.815643
267.724030	8000.440083	14.045594	-0.054969	4.815650
267.612042	8000.370955	14.050599	-0.054948	4.815630
267.721349	8000.421881	14.055603	-0.054969	4.815645
267.603264	8000.357994	14.060608	-0.054947	4.815626
267.491425	8000.403161	14.065613	-0.054926	4.815640
267.564091	8000.436397	14.070618	-0.054939	4.815650
267.536322	8000.451965	14.075623	-0.054934	4.815654
267.568715	8000.486677	14.080627	-0.054940	4.815664
267.537316	8000.409255	14.085632	-0.054934	4.815642
267.682101	8000.376378	14.090637	-0.054961	4.815631
267.626825	8000.428881	14.095642	-0.054951	4.815647
267.557826	8000.397843	14.100647	-0.054938	4.815638
267.757400	8000.429952	14.105651	-0.054975	4.815647
267.654034	8000.382329	14.110656	-0.054956	4.815633
267.702785	8000.436536	14.115661	-0.054965	4.815649
267.750980	8000.462961	14.120666	-0.054974	4.815656
267.590025	8000.424008	14.125671	-0.054944	4.815646
267.799723	8000.497942	14.130675	-0.054983	4.815666
267.498938	8000.454561	14.135680	-0.054927	4.815655
267.627702	8000.448126	14.140685	-0.054951	4.815653
267.684469	8000.442647	14.145690	-0.054962	4.815651
267.490451	8000.404220	14.150695	-0.054926	4.815641
267.674730	8000.442488	14.155699	-0.054960	4.815651
267.873380	8000.454288	14.160704	-0.054997	4.815653
267.798175	8000.377216	14.165709	-0.054983	4.815631
267.704506	8000.388501	14.170714	-0.054966	4.815635
267.689326	8000.414956	14.175719	-0.054963	4.815643
267.770240	8000.456872	14.180723	-0.054978	4.815655
267.727217	8000.451895	14.185728	-0.054970	4.815653
267.906773	8000.387542	14.190733	-0.055003	4.815634
267.691322	8000.402173	14.195738	-0.054963	4.815639
267.567462	8000.401213	14.200743	-0.054940	4.815639
267.643942	8000.445192	14.205747	-0.054954	4.815652
267.589519	8000.366325	14.210752	-0.054944	4.815629
267.649617	8000.442081	14.215757	-0.054955	4.815651
267.650002	8000.437815	14.220762	-0.054955	4.815650
267.683679	8000.427686	14.225767	-0.054962	4.815646
267.766741	8000.432251	14.230771	-0.054977	4.815647
267.644618	8000.391797	14.235776	-0.054954	4.815636
267.798123	8000.397516	14.240781	-0.054983	4.815637
267.818953	8000.472630	14.245786	-0.054987	4.815659
267.535678	8000.388946	14.250791	-0.054934	4.815636
267.610668	8000.379493	14.255795	-0.054948	4.815633
267.574579	7999.343892	14.260800	-0.054941	4.815330
267.708621	7996.145323	14.265805	-0.054964	4.814395
267.667331	7990.674796	14.270810	-0.054952	4.812795
267.534198	7983.914477	14.275815	-0.054923	4.810818
267.643843	7976.630710	14.280819	-0.054939	4.808686
267.351452	7968.986710	14.285824	-0.054879	4.806450
267.377129	7961.179728	14.290829	-0.054879	4.804163
267.478334	7953.388264	14.295834	-0.054893	4.801879
267.276240	7945.357449	14.300839	-0.054850	4.799525
267.415095	7937.467664	14.305843	-0.054871	4.797210
267.471806	7929.379432	14.310848	-0.054876	4.794836
267.379047	7921.383386	14.315853	-0.054854	4.792489
267.145421	7913.402040	14.320858	-0.054805	4.790145
267.026983	7905.377471	14.325863	-0.054778	4.787787
267.125338	7897.397068	14.330867	-0.054791	4.785440
267.044432	7889.412793	14.335872	-0.054770	4.783091
267.105028	7881.404698	14.340877	-0.054776	4.780734
267.319905	7873.441807	14.345882	-0.054811	4.778388
267.097723	7865.409225	14.350887	-0.054765	4.776022
267.026550	7857.405961	14.355891	-0.054746	4.773663
266.954190	7849.337886	14.360896	-0.054728	4.771284
267.073789	7841.373589	14.365901	-0.054745	4.768933
267.009168	7833.377079	14.370906	-0.054727	4.766573
266.856436	7825.382436	14.375911	-0.054694	4.764212
266.728643	7817.418526	14.380915	-0.054665	4.761859
266.507216	7809.349833	14.385920	-0.054618	4.759474
266.621978	7801.412612	14.390925	-0.054634	4.757126
266.697676	7793.393409	14.395930	-0.054643	4.754752
266.542487	7785.270205	14.400935	-0.054609	4.752347
266.525135	7777.339169	14.405939	-0.054601	4.749998
266.663924	7769.341098	14.410944	-0.054621	4.747626
266.719987	7761.295584	14.415949	-0.054627	4.745240
266.690077	7753.337365	14.420954	-0.054616	4.742879
266.451380	7745.300040	14.425959	-0.054566	4.740494
266.686274	7737.404014	14.430963	-0.054605	4.738148
266.607205	7729.329121	14.435968	-0.054585	4.735749
266.404399	7721.329607	14.440973	-0.054542	4.733371
266.451851	7713.289339	14.445978	-0.054545	4.730979
266.463198	7705.272722	14.450983	-0.054542	4.728593
266.321381	7697.280783	14.455987	-0.054511	4.726214
266.091215	7689.336154	14.460992	-0.054463	4.723848
266.235670	7681.283654	14.465997	-0.054484	4.721448
266.405417	7673.325428	14.471002	-0.054511	4.719074
266.247432	7665.349610	14.476007	-0.054476	4.716695
266.279250	7657.292634	14.481011	-0.054477	4.714289
266.095282	7649.285094	14.486016	-0.054437	4.711898
265.906249	7641.243012	14.491021	-0.054397	4.709496
265.982386	7633.322983	14.496026	-0.054406	4.707128
265.897708	7625.271140	14.501031	-0.054385	4.704719
266.210314	7617.343091	14.506035	-0.054438	4.702346
265.885264	7609.276930	14.511040	-0.054372	4.699931
265.805479	7601.324006	14.516045	-0.054352	4.697549
265.715276	7593.331352	14.521050	-0.054330	4.695153
265.671250	7585.274421	14.526055	-0.054317	4.692737
265.896967	7577.268051	14.531059	-0.054354	4.690335
265.899909	7569.279977	14.536064	-0.054349	4.687937
265.712572	7561.239828	14.541069	-0.054309	4.685522
265.822661	7553.342657	14.546074	-0.054324	4.683149
265.830345	7545.286960	14.551079	-0.054320	4.680727
265.841445	7537.348552	14.556083	-0.054317	4.678339
265.586643	7529.271841	14.561088	-0.054264	4.675908
265.469145	7521.203202	14.566093	-0.054237	4.673479
265.701815	7513.164246	14.571098	-0.054275	4.671056
265.381639	7505.142483	14.576103	-0.054211	4.668639
265.602537	7497.218346	14.581107	-0.054247	4.666248
265.498746	7489.230696	14.586112	-0.054222	4.663838
265.415645	7481.229726	14.591117	-0.054201	4.661423
265.251233	7473.263649	14.596122	-0.054166	4.659017
265.271969	7465.288967	14.601127	-0.054164	4.656606
265.305303	7457.255491	14.606131	-0.054165	4.654177
265.390238	7449.179937	14.611136	-0.054176	4.651734
265.389838	7441.173319	14.616141	-0.054170	4.649310
265.195945	7433.202320	14.621146	-0.054129	4.646896
265.276778	7425.190899	14.626151	-0.054139	4.644469
265.129937	7417.287109	14.631155	-0.054107	4.642072
265.109367	7409.167528	14.636160	-0.054097	4.639610
265.208573	7401.243785	14.641165	-0.054111	4.637205
265.189305	7393.261222	14.646170	-0.054102	4.634781
265.176475	7385.176018	14.651175	-0.054094	4.632324
265.062397	7377.155565	14.656179	-0.054068	4.629886
264.988708	7369.175353	14.661184	-0.054049	4.627459
265.079041	7361.144125	14.666189	-0.054060	4.625015
265.223846	7353.253501	14.671194	-0.054082	4.622613
264.916096	7345.192510	14.676199	-0.054020	4.620158
264.977022	7337.209785	14.681203	-0.054026	4.617725
264.908720	7329.164706	14.686208	-0.054008	4.615271
264.808699	7321.162814	14.691213	-0.053984	4.612830
264.649014	7313.156020	14.696218	-0.053949	4.610386
264.655491	7305.153467	14.701223	-0.053945	4.607941
264.715233	7297.172495	14.706227	-0.053951	4.605503
264.686201	7289.187644	14.711232	-0.053940	4.603061
264.685915	7281.171310	14.716237	-0.053935	4.600609
264.571304	7273.213443	14.721242	-0.053909	4.598173
264.279388	7265.186718	14.726247	-0.053849	4.595715
264.329590	7257.168950	14.731251	-0.053853	4.593258
264.320059	7249.084303	14.736256	-0.053846	4.590780
264.493110	7241.095247	14.741261	-0.053873	4.588329
264.521943	7233.090376	14.746266	-0.053873	4.585872
264.362481	7225.087193	14.751271	-0.053838	4.583415
264.336752	7217.146949	14.756275	-0.053829	4.580975
264.166719	7209.140279	14.761280	-0.053792	4.578514
264.124462	7201.146743	14.766285	-0.053779	4.576055
264.096645	7193.129084	14.771290	-0.053768	4.573588
264.133885	7185.080072	14.776295	-0.053770	4.571110
264.227165	7177.127417	14.781299	-0.053782	4.568660
264.113888	7169.140281	14.786304	-0.053756	4.566198
264.155861	7161.086051	14.791309	-0.053758	4.563714
264.050353	7153.162233	14.796314	-0.053734	4.561269
263.977491	7145.162706	14.801319	-0.053715	4.558799
264.022052	7137.170052	14.806323	-0.053718	4.556330
263.911422	7129.129939	14.811328	-0.053692	4.553845
264.070547	7121.092944	14.816333	-0.053716	4.551360
264.003551	7113.108850	14.821338	-0.053699	4.548889
263.542825	7105.078785	14.826343	-0.053608	4.546403
263.642848	7097.130835	14.831347	-0.053621	4.543941
263.682306	7089.129095	14.836352	-0.053623	4.541461
263.728084	7081.095446	14.841357	-0.053627	4.538970
263.695385	7073.148158	14.846362	-0.053615	4.536504
263.697426	7065.095403	14.851367	-0.053610	4.534005
263.873137	7057.065067	14.856371	-0.053638	4.531511
263.593078	7049.086313	14.861376	-0.053581	4.529031
263.676178	7041.115585	14.866381	-0.053591	4.526552
263.724460	7033.130381	14.871386	-0.053595	4.524068
263.645619	7025.102343	14.876391	-0.053575	4.521569
263.571003	7017.139881	14.881395	-0.053556	4.519089
263.347123	7009.150914	14.886400	-0.053509	4.516599
263.460596	7001.057708	14.891405	-0.053525	4.514076
263.500683	6993.033607	14.896410	-0.053527	4.511572
263.357131	6984.998459	14.901415	-0.053495	4.509064
263.356153	6977.052593	14.906419	-0.053490	4.506582
263.320866	6969.058472	14.911424	-0.053478	4.504084
263.369232	6961.079054	14.916429	-0.053482	4.501589
263.405605	6953.090189	14.921434	-0.053483	4.499090
263.216483	6945.065946	14.926439	-0.053443	4.496578
263.206797	6937.040604	14.931443	-0.053436	4.494064
263.069599	6929.038910	14.936448	-0.053405	4.491556
263.152382	6921.046571	14.941453	-0.053415	4.489051
263.072595	6913.064266	14.946458	-0.053395	4.486546
263.023544	6905.043390	14.951463	-0.053381	4.484028
263.191786	6897.058591	14.956467	-0.053407	4.481521
262.933744	6889.061831	14.961472	-0.053354	4.479007
262.750853	6881.046034	14.966477	-0.053314	4.476486
262.937447	6873.087350	14.971482	-0.053344	4.473983
262.692116	6865.006971	14.976487	-0.053293	4.471438
262.644493	6857.056894	14.981491	-0.053279	4.468934
262.775066	6849.026061	14.986496	-0.053298	4.466404
262.694859	6841.014076	14.991501	-0.053278	4.463877
262.516998	6833.058280	14.996506	-0.053240	4.461367
262.648668	6824.998501	15.001511	-0.053259	4.458823
262.687659	6817.055086	15.006515	-0.053261	4.456314
262.592037	6808.986467	15.011520	-0.053238	4.453764
262.679296	6800.957708	15.016525	-0.053249	4.451225
262.685619	6792.991756	15.021530	-0.053245	4.448705
262.481481	6784.961099	15.026535	-0.053202	4.446161
262.460257	6777.036164	15.031539	-0.053193	4.443651
262.185709	6769.047237	15.036544	-0.053136	4.441118
262.266553	6761.009919	15.041549	-0.053146	4.438569
262.248093	6753.013976	15.046554	-0.053137	4.436032
262.104820	6744.966371	15.051559	-0.053105	4.433476
262.338700	6736.948571	15.056563	-0.053144	4.430930
262.113182	6728.940928	15.061568	-0.053097	4.428384
262.048667	6720.921900	15.066573	-0.053079	4.425833
262.064588	6713.027957	15.071578	-0.053077	4.423322
261.886310	6704.981631	15.076583	-0.053039	4.420759
261.928681	6696.993522	15.081587	-0.053041	4.418214
261.968982	6688.967938	15.086592	-0.053044	4.415656
261.941929	6680.949023	15.091597	-0.053033	4.413098
261.913747	6672.983692	15.096602	-0.053023	4.410556
261.863007	6664.973486	15.101607	-0.053008	4.407997
261.899796	6656.955800	15.106611	-0.053010	4.405436
261.844127	6648.984307	15.111616	-0.052994	4.402887
261.527949	6640.972982	15.116621	-0.052930	4.400323
261.708512	6633.023487	15.121626	-0.052959	4.397779
261.493450	6624.992638	15.126631	-0.052913	4.395206
261.569061	6616.968430	15.131635	-0.052922	4.392635
261.470560	6608.936337	15.136640	-0.052899	4.390059
261.602027	6600.941949	15.141645	-0.052918	4.387495
261.488216	6592.957501	15.146650	-0.052892	4.384931
261.464581	6584.987824	15.151655	-0.052882	4.382371
261.551993	6576.982940	15.156659	-0.052893	4.379799
261.563625	6568.982176	15.161664	-0.052890	4.377226
261.349183	6560.991263	15.166669	-0.052845	4.374654
261.417936	6553.002769	15.171674	-0.052853	4.372082
261.261943	6544.936967	15.176679	-0.052818	4.369483
261.228615	6536.974396	15.181683	-0.052807	4.366916
261.141912	6528.992396	15.186688	-0.052786	4.364341
261.256007	6520.990938	15.191693	-0.052802	4.361759
261.332488	6512.980420	15.196698	-0.052811	4.359173
261.184480	6505.028346	15.201703	-0.052778	4.356602
261.191173	6496.964023	15.206707	-0.052774	4.353995
261.009481	6488.867821	15.211712	-0.052735	4.351375
261.068650	6480.855548	15.216717	-0.052741	4.348782
261.039639	6472.947182	15.221722	-0.052730	4.346220
260.902553	6464.943659	15.226727	-0.052699	4.343626
260.749878	6456.962634	15.231731	-0.052666	4.341036
260.757622	6448.972461	15.236736	-0.052662	4.338444
260.869510	6440.965617	15.241741	-0.052677	4.335845
260.977594	6432.975148	15.246746	-0.052692	4.333250
260.675162	6424.913866	15.251751	-0.052631	4.330628
260.770552	6416.957297	15.256755	-0.052643	4.328040
260.723174	6408.967380	15.261760	-0.052629	4.325440
260.501502	6400.953601	15.266765	-0.052583	4.322829
260.597884	6392.968247	15.271770	-0.052596	4.320227
260.693318	6384.954189	15.276775	-0.052608	4.317615
260.521177	6376.951082	15.281779	-0.052571	4.315003
260.454242	6368.919872	15.286784	-0.052553	4.312381
260.442656	6360.868404	15.291789	-0.052546	4.309751
260.431904	6352.960309	15.296794	-0.052539	4.307166
260.301896	6344.895649	15.301799	-0.052509	4.304528
260.281678	6336.952593	15.306803	-0.052500	4.301928
260.223386	6328.921857	15.311808	-0.052484	4.299298
260.454424	6320.930006	15.316813	-0.052522	4.296682
260.430636	6312.929180	15.321818	-0.052512	4.294059
260.180420	6304.844652	15.326823	-0.052461	4.291405
260.153290	6296.900415	15.331827	-0.052450	4.288797
260.192607	6288.909000	15.336832	-0.052452	4.286173
260.160049	6280.898644	15.341837	-0.052441	4.283540
260.204794	6272.935876	15.346842	-0.052444	4.280922
260.208671	6264.972376	15.351847	-0.052440	4.278301
260.188900	6256.909151	15.356851	-0.052431	4.275646
260.225516	6248.903482	15.361856	-0.052433	4.273009
260.032967	6240.817866	15.366861	-0.052391	4.270342
260.016294	6232.924815	15.371866	-0.052383	4.267738
259.810082	6224.843064	15.376871	-0.052339	4.265069
259.816085	6216.938436	15.381875	-0.052335	4.262458
259.734241	6208.907864	15.386880	-0.052315	4.259804
259.927954	6200.936200	15.391885	-0.052346	4.257169
260.029228	6192.915335	15.396890	-0.052360	4.254516
259.667963	6184.844319	15.401895	-0.052287	4.251841
259.794515	6176.854491	15.406899	-0.052305	4.249195
259.819350	6168.876206	15.411904	-0.052305	4.246550
259.898425	6160.873136	15.416909	-0.052314	4.243896
259.794274	6152.935717	15.421914	-0.052290	4.241261
259.733580	6144.940021	15.426919	-0.052273	4.238604
259.585525	6136.941549	15.431923	-0.052240	4.235945
259.752215	6128.913728	15.436928	-0.052266	4.233277
259.512497	6120.853966	15.441933	-0.052216	4.230592
259.726358	6112.919233	15.446938	-0.052251	4.227953
259.471230	6104.868322	15.451943	-0.052198	4.225268
259.512733	6096.933656	15.456947	-0.052201	4.222623
259.592785	6088.912989	15.461952	-0.052211	4.219948
259.219607	6080.937194	15.466957	-0.052136	4.217282
259.253884	6072.926236	15.471962	-0.052137	4.214606
259.233602	6064.904281	15.476967	-0.052128	4.211924
259.324519	6056.938164	15.481971	-0.052140	4.209261
259.210401	6048.921836	15.486976	-0.052113	4.206577
259.233550	6040.946491	15.491981	-0.052112	4.203907
259.219320	6032.954096	15.496986	-0.052105	4.201228
259.042190	6024.961693	15.501991	-0.052066	4.198546
258.878951	6016.982408	15.506995	-0.052031	4.195867
259.012656	6008.842676	15.512000	-0.052050	4.193136
259.001599	6000.804803	15.517005	-0.052043	4.190435
258.963859	5992.852824	15.522010	-0.052031	4.187762
258.798713	5984.864613	15.527015	-0.051995	4.185073
258.795763	5976.920829	15.532019	-0.051989	4.182399
258.984366	5968.889681	15.537024	-0.052019	4.179696
258.799550	5960.914866	15.542029	-0.051979	4.177006
258.909916	5952.908643	15.547034	-0.051995	4.174307
258.738011	5944.867965	15.552039	-0.051958	4.171591
258.851899	5936.910806	15.557043	-0.051974	4.168905
258.666654	5928.894024	15.562048	-0.051934	4.166194
258.639048	5920.883652	15.567053	-0.051924	4.163485
258.475299	5912.915444	15.572058	-0.051888	4.160787
258.572814	5904.890967	15.577063	-0.051901	4.158071
258.791342	5896.887788	15.582067	-0.051936	4.155363
258.756493	5888.895782	15.587072	-0.051925	4.152653
258.559782	5880.839229	15.592077	-0.051883	4.149917
258.580130	5872.877908	15.597082	-0.051881	4.147215
258.518174	5864.861287	15.602087	-0.051865	4.144491
258.407688	5856.915044	15.607091	-0.051839	4.141788
258.293614	5848.886083	15.612096	-0.051812	4.139056
258.245737	5840.873857	15.617101	-0.051798	4.136328
258.167218	5832.911117	15.622106	-0.051778	4.133615
258.074351	5824.811312	15.627111	-0.051756	4.130854
258.107031	5816.897243	15.632115	-0.051757	4.128155
258.165006	5808.896880	15.637120	-0.051762	4.125425
257.973445	5800.925613	15.642125	-0.051721	4.122701
258.011124	5792.878146	15.647130	-0.051723	4.119951
257.854927	5784.915365	15.652135	-0.051689	4.117226
257.978584	5776.891815	15.657139	-0.051707	4.114482
258.046043	5768.876600	15.662144	-0.051714	4.111739
257.932676	5760.825278	15.667149	-0.051688	4.108979
257.857168	5752.878108	15.672154	-0.051669	4.106253
257.738295	5744.887880	15.677159	-0.051641	4.103510
257.789795	5736.881055	15.682163	-0.051646	4.100761
257.798852	5728.897574	15.687168	-0.051642	4.098019
257.482766	5720.837641	15.692173	-0.051578	4.095244
257.635807	5712.892029	15.697178	-0.051601	4.092512
257.570874	5704.894930	15.702183	-0.051584	4.089758
257.485539	5696.948448	15.707187	-0.051563	4.087020
257.375586	5688.902382	15.712192	-0.051537	4.084245
257.456456	5680.917583	15.717197	-0.051547	4.081491
257.352828	5672.935572	15.722202	-0.051523	4.078735
257.331343	5664.950288	15.727207	-0.051513	4.075976
257.413154	5656.913892	15.732211	-0.051523	4.073199
257.249624	5648.875750	15.737216	-0.051488	4.070417
257.227084	5640.914980	15.742221	-0.051478	4.067661
257.502082	5632.923121	15.747226	-0.051524	4.064897
257.446499	5624.919565	15.752231	-0.051509	4.062122
257.204264	5616.920221	15.757235	-0.051458	4.059344
257.142481	5608.973822	15.762240	-0.051442	4.056585
257.204742	5600.909079	15.767245	-0.051448	4.053785
257.265766	5592.920880	15.772250	-0.051454	4.051009
257.063802	5584.920488	15.777255	-0.051411	4.048224
257.062367	5576.925287	15.782259	-0.051406	4.045441
257.062356	5568.942704	15.787264	-0.051401	4.042661
256.864043	5560.916768	15.792269	-0.051359	4.039861
256.849053	5552.999594	15.797274	-0.051351	4.037099
256.876513	5544.915221	15.802279	-0.051351	4.034278
256.850948	5536.830749	15.807283	-0.051340	4.031455
256.838559	5528.851403	15.812288	-0.051333	4.028666
256.665396	5520.840882	15.817293	-0.051296	4.025862
256.928911	5512.911413	15.822298	-0.051339	4.023090
256.557843	5504.894039	15.827303	-0.051265	4.020277
256.649617	5496.937673	15.832307	-0.051277	4.017490
256.731597	5488.905362	15.837312	-0.051287	4.014674
256.588518	5480.870021	15.842317	-0.051255	4.011852
256.707078	5472.910438	15.847322	-0.051272	4.009058
256.709778	5464.909179	15.852327	-0.051267	4.006246
256.633952	5456.948150	15.857331	-0.051248	4.003445
256.531290	5448.922120	15.862336	-0.051224	4.000619
256.488509	5440.928327	15.867341	-0.051211	3.997803
256.718550	5432.899373	15.872346	-0.051248	3.994977
256.302187	5424.866777	15.877351	-0.051165	3.992137
256.179272	5416.878709	15.882355	-0.051137	3.989316
256.322046	5408.894643	15.887360	-0.051159	3.986498
256.188517	5400.877812	15.892365	-0.051129	3.983662
256.090249	5392.913635	15.897370	-0.051105	3.980844
256.011597	5384.951581	15.902375	-0.051085	3.978024
256.048037	5376.914015	15.907379	-0.051087	3.975178
256.021249	5368.931853	15.912384	-0.051077	3.972348
255.875168	5360.863402	15.917389	-0.051044	3.969484
255.977376	5352.920004	15.922394	-0.051058	3.966666
255.975722	5344.897572	15.927399	-0.051053	3.963816
255.898152	5336.955681	15.932403	-0.051033	3.960992
256.023060	5328.979015	15.937408	-0.051051	3.958156
255.727905	5320.979282	15.942413	-0.050991	3.955303
255.638986	5312.964029	15.947418	-0.050969	3.952446
255.588863	5304.912453	15.952423	-0.050954	3.949575
255.831679	5296.916251	15.957427	-0.050994	3.946727
255.477955	5288.958595	15.962432	-0.050923	3.943879
255.466720	5280.919158	15.967437	-0.050916	3.941007
255.793804	5272.978788	15.972442	-0.050972	3.938174
255.575985	5264.979561	15.977447	-0.050926	3.935308
255.330391	5256.989393	15.982451	-0.050875	3.932442
255.580602	5248.983751	15.987456	-0.050917	3.929578
255.538670	5240.964628	15.992461	-0.050903	3.926702
255.386442	5232.983077	15.997466	-0.050870	3.923835
255.378945	5224.983568	16.002471	-0.050863	3.920962
255.645311	5217.002892	16.007475	-0.050908	3.918099
255.514477	5209.017028	16.012480	-0.050878	3.915224
255.369277	5200.951117	16.017485	-0.050846	3.912319
255.383802	5192.969680	16.022490	-0.050843	3.909444
255.315503	5184.961168	16.027495	-0.050825	3.906556
255.336211	5176.972161	16.032499	-0.050824	3.903675
255.306542	5168.989947	16.037504	-0.050813	3.900793
255.252411	5160.982967	16.042509	-0.050798	3.897900
255.190317	5152.983243	16.047514	-0.050781	3.895007
255.165483	5144.989258	16.052519	-0.050772	3.892114
255.173025	5136.974522	16.057523	-0.050768	3.889212
255.061337	5129.004833	16.062528	-0.050742	3.886323
254.962622	5120.988794	16.067533	-0.050718	3.883414
255.113684	5112.994689	16.072538	-0.050741	3.880516
255.010578	5105.013268	16.077543	-0.050717	3.877616
254.791316	5097.007200	16.082547	-0.050671	3.874702
254.759446	5088.740550	16.087552	-0.050659	3.871695
254.639894	5080.802355	16.092557	-0.050632	3.868804
254.692158	5072.891638	16.097562	-0.050636	3.865923
254.530617	5064.951399	16.102567	-0.050601	3.863026
254.618396	5056.946197	16.107571	-0.050612	3.860107
254.543506	5048.972216	16.112576	-0.050593	3.857195
254.387330	5040.966074	16.117581	-0.050559	3.854267
254.602464	5032.974531	16.122586	-0.050594	3.851349
254.455313	5024.964757	16.127591	-0.050561	3.848415
254.544133	5016.969296	16.132595	-0.050572	3.845489
254.528566	5009.014691	16.137600	-0.050564	3.842574
254.333014	5000.993708	16.142605	-0.050523	3.839628
254.338574	4993.088373	16.147610	-0.050519	3.836727
254.276739	4985.022053	16.152615	-0.050502	3.833763
254.191343	4977.010886	16.157619	-0.050481	3.830817
254.358304	4969.010212	16.162624	-0.050507	3.827877
254.041755	4960.977988	16.167629	-0.050442	3.824913
254.040991	4953.083098	16.172634	-0.050437	3.822004
254.074039	4945.026385	16.177639	-0.050438	3.819034
254.024999	4937.077086	16.182643	-0.050424	3.816100
254.099203	4929.050731	16.187648	-0.050432	3.813138
254.031082	4921.036329	16.192653	-0.050414	3.810174
254.043611	4913.101120	16.197658	-0.050412	3.807240
253.852195	4905.073519	16.202663	-0.050371	3.804264
253.815547	4897.108910	16.207667	-0.050359	3.801313
253.948287	4889.110227	16.212672	-0.050378	3.798350
253.809253	4881.079122	16.217677	-0.050347	3.795367
253.840527	4873.057747	16.222682	-0.050348	3.792390
253.639336	4865.008625	16.227687	-0.050305	3.789394
253.600241	4857.062018	16.232691	-0.050293	3.786438
253.592007	4849.048523	16.237696	-0.050286	3.783455
253.485412	4841.098372	16.242701	-0.050261	3.780491
253.617082	4833.090757	16.247706	-0.050280	3.777509
253.482636	4825.081245	16.252711	-0.050250	3.774518
253.530891	4817.073753	16.257715	-0.050254	3.771529
253.469358	4809.078438	16.262720	-0.050237	3.768540
253.443941	4801.033887	16.267725	-0.050227	3.765531
253.417718	4793.092559	16.272730	-0.050217	3.762559
253.474769	4785.101585	16.277735	-0.050222	3.759567
253.314733	4777.127832	16.282739	-0.050187	3.756574
253.327304	4769.105754	16.287744	-0.050184	3.753565
253.312481	4761.051081	16.292749	-0.050176	3.750540
253.204070	4753.103417	16.297754	-0.050151	3.747551
253.088604	4745.097859	16.302759	-0.050124	3.744538
253.196348	4737.107221	16.307763	-0.050139	3.741533
253.094737	4729.140247	16.312768	-0.050115	3.738530
253.039568	4721.130442	16.317773	-0.050100	3.735509
253.083207	4713.116771	16.322778	-0.050103	3.732486
253.033216	4705.079971	16.327783	-0.050088	3.729450
252.868685	4697.125565	16.332787	-0.050052	3.726441
252.887770	4689.165959	16.337792	-0.050051	3.723431
252.958616	4681.163307	16.342797	-0.050059	3.720403
252.796093	4673.226596	16.347802	-0.050023	3.717393
252.620029	4665.139223	16.352807	-0.049985	3.714322
252.843024	4657.057548	16.357811	-0.050021	3.711261
252.881228	4649.106988	16.362816	-0.050023	3.708243
252.488695	4641.099708	16.367821	-0.049945	3.705190
252.514098	4633.168807	16.372826	-0.049945	3.702174
252.378287	4625.182753	16.377831	-0.049914	3.699130
252.446656	4617.184233	16.382835	-0.049922	3.696084
252.420716	4609.184565	16.387840	-0.049912	3.693033
252.521736	4601.153724	16.392845	-0.049925	3.689971
252.352005	4593.202957	16.397850	-0.049888	3.686929
252.157986	4585.215542	16.402855	-0.049847	3.683871
252.350996	4577.190371	16.407859	-0.049878	3.680806
252.551684	4569.216935	16.412864	-0.049910	3.677758
252.241598	4561.209249	16.417869	-0.049847	3.674681
252.360946	4553.204036	16.422874	-0.049864	3.671613
252.419998	4545.203015	16.427879	-0.049870	3.668544
252.378262	4537.195161	16.432883	-0.049857	3.665466
252.406627	4529.233953	16.437888	-0.049857	3.662405
252.170421	4521.211378	16.442893	-0.049808	3.659312
252.108003	4513.289208	16.447898	-0.049791	3.656259
251.939692	4505.231956	16.452903	-0.049754	3.653148
251.921961	4497.222307	16.457907	-0.049746	3.650058
252.110822	4489.252161	16.462912	-0.049776	3.646985
252.029336	4481.224077	16.467917	-0.049755	3.643880
251.776181	4473.290553	16.472922	-0.049703	3.640805
251.790627	4465.279246	16.477927	-0.049701	3.637704
251.854875	4457.245542	16.482931	-0.049707	3.634592
251.893163	4449.218890	16.487936	-0.049709	3.631481
251.918804	4441.220090	16.492941	-0.049709	3.628377
251.745190	4433.225996	16.497946	-0.049671	3.625267
251.605671	4425.288626	16.502951	-0.049640	3.622177
251.586131	4417.256634	16.507955	-0.049631	3.619051
251.651946	4409.299294	16.512960	-0.049638	3.615953
251.322622	4401.316644	16.517965	-0.049572	3.612833
251.306890	4393.282017	16.522970	-0.049564	3.609698
251.270848	4385.316564	16.527975	-0.049552	3.606586
251.314261	4377.285271	16.532979	-0.049555	3.603449
251.385648	4369.322782	16.537984	-0.049563	3.600336
251.262647	4361.366738	16.542989	-0.049535	3.597218
251.311619	4353.348749	16.547994	-0.049538	3.594077
251.250620	4345.328171	16.552999	-0.049522	3.590930
251.372962	4337.328442	16.558003	-0.049539	3.587793
251.314318	4329.353536	16.563008	-0.049523	3.584659
251.374791	4321.373018	16.568013	-0.049529	3.581522
251.271738	4313.391556	16.573018	-0.049505	3.578378
251.261961	4305.392129	16.578023	-0.049498	3.575227
251.192991	4297.373230	16.583027	-0.049480	3.572063
251.053742	4289.418824	16.588032	-0.049449	3.568920
250.883727	4281.369464	16.593037	-0.049412	3.565736
251.019966	4273.411344	16.598042	-0.049432	3.562594
251.082837	4265.397001	16.603047	-0.049439	3.559425
250.876917	4257.456204	16.608051	-0.049395	3.556274
251.134813	4249.358142	16.613056	-0.049438	3.553072
250.896470	4241.309780	16.618061	-0.049388	3.549872
250.822269	4233.363396	16.623066	-0.049369	3.546714
250.664911	4225.387962	16.628071	-0.049335	3.543540
250.748106	4217.397751	16.633075	-0.049345	3.540364
250.811651	4209.430266	16.638080	-0.049352	3.537193
250.580638	4201.406015	16.643085	-0.049303	3.533989
250.600616	4193.423344	16.648090	-0.049302	3.530805
250.422183	4185.451210	16.653095	-0.049263	3.527617
250.541966	4177.419157	16.658099	-0.049281	3.524411
250.633851	4169.476074	16.663104	-0.049293	3.521237
250.519370	4161.443655	16.668109	-0.049266	3.518018
250.373021	4153.481836	16.673114	-0.049234	3.514823
250.431376	4145.447785	16.678119	-0.049239	3.511603
250.323797	4137.449421	16.683123	-0.049214	3.508389
250.201585	4129.499958	16.688128	-0.049186	3.505191
250.148049	4121.502830	16.693133	-0.049171	3.501973
250.436342	4113.507465	16.698138	-0.049219	3.498763
250.284333	4105.523385	16.703143	-0.049186	3.495542
250.246809	4097.532388	16.708147	-0.049174	3.492318
250.116325	4089.535965	16.713152	-0.049144	3.489086
250.177246	4081.525052	16.718157	-0.049150	3.485851
249.959705	4073.603636	16.723162	-0.049105	3.482641
249.813385	4065.566063	16.728167	-0.049072	3.479383
250.078905	4057.565166	16.733171	-0.049116	3.476150
249.964473	4049.578606	16.738176	-0.049090	3.472907
249.793935	4041.536368	16.743181	-0.049053	3.469637
249.757664	4033.584040	16.748186	-0.049041	3.466405
249.804238	4025.562714	16.753191	-0.049044	3.463145
249.710004	4017.576288	16.758195	-0.049022	3.459890
249.737209	4009.639766	16.763200	-0.049021	3.456658
249.607426	4001.585552	16.768205	-0.048992	3.453369
249.560284	3993.610388	16.773210	-0.048978	3.450111
249.412951	3985.622618	16.778215	-0.048945	3.446843
249.542445	3977.615510	16.783219	-0.048964	3.443572
249.764599	3969.609199	16.788224	-0.049001	3.440302
249.488282	3961.669222	16.793229	-0.048944	3.437039
249.737009	3953.638574	16.798234	-0.048985	3.433753
249.646165	3945.634131	16.803239	-0.048963	3.430464
249.630819	3937.646415	16.808243	-0.048955	3.427181
249.539407	3929.684748	16.813248	-0.048933	3.423903
249.373876	3921.679256	16.818253	-0.048897	3.420601
249.476347	3913.713223	16.823258	-0.048910	3.417321
249.220801	3905.699681	16.828263	-0.048858	3.414007
249.210037	3897.675268	16.833267	-0.048850	3.410693
249.283653	3889.712050	16.838272	-0.048859	3.407404
249.126737	3881.700266	16.843277	-0.048824	3.404083
249.221723	3873.754468	16.848282	-0.048837	3.400796
249.160220	3865.788003	16.853287	-0.048820	3.397491
248.982609	3857.768370	16.858291	-0.048782	3.394157
249.067101	3849.669318	16.863296	-0.048793	3.390796
248.982507	3841.698327	16.868301	-0.048772	3.387479
248.998247	3833.736464	16.873306	-0.048769	3.384166
248.778259	3825.765640	16.878311	-0.048723	3.380838
248.779599	3817.793728	16.883315	-0.048718	3.377513
248.927762	3809.804480	16.888320	-0.048741	3.374184
248.695688	3801.761351	16.893325	-0.048692	3.370815
248.692183	3793.818768	16.898330	-0.048686	3.367493
248.885110	3785.809827	16.903335	-0.048717	3.364146
248.724364	3777.836872	16.908339	-0.048682	3.360799
248.738370	3769.876256	16.913344	-0.048679	3.357460
248.710723	3761.832772	16.918349	-0.048669	3.354082
248.697684	3753.807284	16.923354	-0.048661	3.350708
248.464186	3745.849018	16.928359	-0.048613	3.347351
248.532521	3737.830439	16.933363	-0.048620	3.343976
248.678462	3729.892372	16.938368	-0.048642	3.340634
248.285859	3721.912249	16.943373	-0.048564	3.337252
248.390960	3713.898423	16.948378	-0.048578	3.333870
248.266644	3705.876607	16.953383	-0.048550	3.330473
248.212353	3697.893014	16.958387	-0.048535	3.327091
248.098509	3689.933112	16.963392	-0.048508	3.323714
248.117739	3681.939476	16.968397	-0.048507	3.320324
248.113258	3673.991365	16.973402	-0.048501	3.316949
248.003776	3665.982828	16.978407	-0.048475	3.313540
247.935743	3657.928312	16.983411	-0.048457	3.310111
248.150350	3649.960354	16.988416	-0.048492	3.306725
247.694838	3641.967202	16.993421	-0.048402	3.303299
247.777888	3633.988591	16.998426	-0.048412	3.299897
247.780263	3626.027580	17.003431	-0.048407	3.296495
247.746282	3618.012389	17.008435	-0.048396	3.293066
247.833425	3610.001974	17.013440	-0.048407	3.289640
247.753270	3602.042594	17.018445	-0.048387	3.286225
247.760133	3594.079314	17.023450	-0.048383	3.282809
247.553453	3586.056452	17.028455	-0.048339	3.279355
247.836652	3578.087024	17.033459	-0.048387	3.275939
247.921538	3570.085059	17.038464	-0.048397	3.272498
247.736404	3562.096489	17.043469	-0.048357	3.269049
247.560449	3554.112713	17.048474	-0.048320	3.265599
247.419940	3546.136392	17.053479	-0.048288	3.262149
247.510816	3538.122124	17.058483	-0.048300	3.258689
247.408662	3530.160725	17.063488	-0.048276	3.255240
247.381588	3522.133197	17.068493	-0.048265	3.251762
247.219617	3514.158369	17.073498	-0.048230	3.248297
247.163124	3506.160106	17.078503	-0.048214	3.244823
247.031793	3498.203935	17.083507	-0.048185	3.241361
247.192366	3490.217069	17.088512	-0.048209	3.237893
247.127999	3482.207999	17.093517	-0.048192	3.234402
246.998843	3474.169266	17.098522	-0.048163	3.230893
247.002700	3466.174111	17.103527	-0.048158	3.227403
247.084404	3458.183181	17.108531	-0.048168	3.223915
246.970885	3450.212735	17.113536	-0.048142	3.220425
246.864966	3442.226758	17.118541	-0.048117	3.216924
246.846363	3434.241315	17.123546	-0.048109	3.213423
246.773556	3426.271120	17.128551	-0.048090	3.209922
246.739773	3418.274008	17.133555	-0.048078	3.206408
246.969849	3410.279862	17.138560	-0.048116	3.202902
246.719748	3402.312267	17.143565	-0.048064	3.199384
246.603567	3394.361365	17.148570	-0.048037	3.195875
246.572951	3386.335437	17.153575	-0.048026	3.192332
246.482926	3378.314217	17.158579	-0.048004	3.188785
246.568505	3370.323984	17.163584	-0.048015	3.185255
246.508381	3362.382610	17.168589	-0.047999	3.181737
246.503814	3354.384170	17.173594	-0.047993	3.178192
246.345469	3346.398907	17.178599	-0.047958	3.174642
246.319059	3338.398697	17.183603	-0.047948	3.171088
246.487481	3330.399881	17.188608	-0.047974	3.167538
246.309045	3322.398666	17.193613	-0.047936	3.163968
246.463349	3314.428911	17.198618	-0.047959	3.160423
246.276973	3306.480851	17.203623	-0.047919	3.156869
246.273550	3298.484907	17.208627	-0.047913	3.153297
246.043233	3290.471323	17.213632	-0.047865	3.149703
246.056573	3282.468970	17.218637	-0.047863	3.146121
246.310993	3274.480656	17.223642	-0.047905	3.142551
246.099835	3266.517087	17.228647	-0.047860	3.138969
245.776987	3258.548003	17.233651	-0.047795	3.135374
246.005044	3250.569323	17.238656	-0.047832	3.131796
246.009869	3242.537150	17.243661	-0.047828	3.128179
245.930163	3234.554465	17.248666	-0.047808	3.124577
245.921108	3226.610668	17.253671	-0.047801	3.120991
245.915279	3218.621134	17.258675	-0.047795	3.117381
246.058093	3210.595723	17.263680	-0.047816	3.113757
245.898744	3202.590417	17.268685	-0.047781	3.110124
245.950878	3194.634669	17.273690	-0.047786	3.106519
245.734383	3186.661402	17.278695	-0.047740	3.102890
245.620068	3178.671540	17.283699	-0.047714	3.099254
245.832402	3170.693959	17.288704	-0.047748	3.095633
245.692836	3162.687739	17.293709	-0.047717	3.091980
245.487084	3154.721673	17.298714	-0.047673	3.088337
245.558215	3146.712539	17.303719	-0.047681	3.084683
245.548288	3138.755873	17.308723	-0.047674	3.081045
245.565413	3130.779965	17.313728	-0.047672	3.077395
245.147437	3122.788960	17.318733	-0.047589	3.073713
245.204881	3114.708339	17.323738	-0.047595	3.070009
245.241094	3106.735380	17.328743	-0.047596	3.066348
245.169417	3098.763958	17.333747	-0.047578	3.062678
245.268267	3090.799574	17.338752	-0.047591	3.059015
245.119929	3082.829432	17.343757	-0.047558	3.055334
244.961122	3074.849095	17.348762	-0.047523	3.051643
245.039355	3066.854090	17.353767	-0.047533	3.047952
245.126168	3058.855708	17.358771	-0.047544	3.044255
245.043901	3050.930947	17.363776	-0.047523	3.040580
244.770425	3042.950179	17.368781	-0.047467	3.036865
244.821400	3034.928865	17.373786	-0.047471	3.033142
244.894488	3026.907023	17.378791	-0.047480	3.029416
244.632623	3018.947319	17.383795	-0.047426	3.025697
244.659716	3010.997513	17.388800	-0.047426	3.021993
244.646927	3002.998099	17.393805	-0.047418	3.018259
244.505622	2995.039409	17.398810	-0.047387	3.014533
244.461111	2987.023794	17.403815	-0.047373	3.010781
244.541035	2979.002456	17.408819	-0.047383	3.007027
244.712306	2971.035359	17.413824	-0.047410	3.003299
244.554493	2963.070258	17.418829	-0.047375	2.999551
244.483046	2955.130622	17.423834	-0.047356	2.995814
244.550593	2947.090120	17.428839	-0.047364	2.992032
244.262257	2939.103451	17.433843	-0.047305	2.988253
244.161511	2931.136193	17.438848	-0.047281	2.984487
244.186907	2923.155053	17.443853	-0.047281	2.980717
244.260641	2915.180823	17.448858	-0.047289	2.976948
244.219829	2907.193332	17.453863	-0.047276	2.973161
244.029725	2899.202420	17.458867	-0.047236	2.969361
243.992738	2891.237608	17.463872	-0.047224	2.965576
244.088153	2883.236621	17.468877	-0.047236	2.961775
244.227131	2875.259512	17.473882	-0.047257	2.957984
244.022337	2867.289046	17.478887	-0.047214	2.954173
243.825315	2859.268670	17.483891	-0.047172	2.950333
243.844485	2851.292229	17.488896	-0.047170	2.946521
243.767174	2843.328737	17.493901	-0.047150	2.942705
243.636290	2835.364508	17.498906	-0.047121	2.938881
243.904026	2827.366713	17.503911	-0.047165	2.935056
243.817282	2819.358742	17.508915	-0.047144	2.931203
243.878276	2811.386719	17.513920	-0.047150	2.927370
243.522801	2803.427903	17.518925	-0.047079	2.923517
243.528718	2795.465408	17.523930	-0.047075	2.919676
243.759941	2787.488022	17.528935	-0.047113	2.915834
243.538636	2779.406948	17.533939	-0.047066	2.911913
243.488550	2771.457147	17.538944	-0.047052	2.908060
243.350316	2763.467170	17.543949	-0.047021	2.904177
243.196769	2755.510842	17.548954	-0.046987	2.900304
243.232941	2747.557054	17.553959	-0.046989	2.896438
243.337208	2739.526877	17.558963	-0.047003	2.892533
243.321673	2731.578376	17.563968	-0.046995	2.888656
243.064358	2723.590784	17.568973	-0.046942	2.884742
243.067673	2715.661052	17.573978	-0.046937	2.880864
243.234146	2707.657510	17.578983	-0.046963	2.876955
243.075629	2699.661653	17.583987	-0.046928	2.873026
243.184360	2691.658317	17.588992	-0.046943	2.869102
243.000790	2683.679637	17.593997	-0.046904	2.865170
243.001464	2675.733123	17.599002	-0.046899	2.861257
242.853575	2667.784463	17.604007	-0.046866	2.857330
242.856116	2659.776125	17.609011	-0.046861	2.853377
242.965251	2651.762420	17.614016	-0.046876	2.849422
242.797790	2643.799286	17.619021	-0.046840	2.845470
242.682257	2635.865331	17.624026	-0.046813	2.841530
242.671395	2627.884047	17.629031	-0.046806	2.837568
242.499791	2619.899573	17.634035	-0.046769	2.833589
242.489015	2611.893665	17.639040	-0.046762	2.829602
242.523938	2603.892575	17.644045	-0.046763	2.825616
242.555240	2595.923169	17.649050	-0.046764	2.821639
242.424204	2587.972344	17.654055	-0.046734	2.817656
242.477141	2579.959377	17.659059	-0.046739	2.813648
242.641356	2571.964924	17.664064	-0.046764	2.809649
242.544268	2563.993201	17.669069	-0.046741	2.805641
242.357215	2556.066254	17.674074	-0.046701	2.801645
242.424724	2548.089097	17.679079	-0.046708	2.797632
242.412199	2540.081255	17.684083	-0.046701	2.793593
242.226415	2532.121142	17.689088	-0.046661	2.789563
242.246195	2524.127797	17.694093	-0.046659	2.785522
242.086702	2516.185982	17.699098	-0.046624	2.781490
241.959034	2508.231147	17.704103	-0.046596	2.777448
241.858299	2500.230769	17.709107	-0.046572	2.773379
241.895674	2492.232796	17.714112	-0.046573	2.769312
241.729879	2484.265430	17.719117	-0.046537	2.765244
241.751498	2476.315426	17.724122	-0.046536	2.761189
241.789105	2468.341014	17.729127	-0.046538	2.757117
241.774870	2460.297881	17.734131	-0.046530	2.753001
241.665866	2452.302302	17.739136	-0.046505	2.748897
241.576917	2444.318180	17.744141	-0.046483	2.744794
241.654746	2436.363961	17.749146	-0.046492	2.740711
241.655197	2428.406472	17.754151	-0.046487	2.736615
241.522423	2420.428282	17.759155	-0.046457	2.732493
241.725486	2412.434997	17.764160	-0.046490	2.728379
241.533682	2404.465642	17.769165	-0.046449	2.724246
241.307358	2396.546334	17.774170	-0.046401	2.720131
241.342209	2388.588112	17.779175	-0.046403	2.716006
241.312571	2380.559585	17.784179	-0.046392	2.711834
241.252177	2372.598081	17.789184	-0.046376	2.707688
241.111063	2364.637529	17.794189	-0.046344	2.703531
241.261188	2356.641757	17.799194	-0.046367	2.699368
241.177661	2348.687539	17.804199	-0.046346	2.695206
241.148658	2340.664592	17.809203	-0.046336	2.691004
241.124750	2332.727950	17.814208	-0.046326	2.686841
241.088032	2324.746352	17.819213	-0.046314	2.682648
240.945710	2316.823852	17.824218	-0.046282	2.678472
241.084459	2308.822248	17.829223	-0.046303	2.674266
241.044649	2300.788025	17.834227	-0.046290	2.670025
240.835070	2292.859858	17.839232	-0.046246	2.665822
240.620493	2284.900125	17.844237	-0.046201	2.661596
240.730826	2276.925856	17.849242	-0.046216	2.657376
240.697539	2268.951780	17.854247	-0.046205	2.653140
240.539843	2260.960815	17.859251	-0.046170	2.648880
240.503178	2253.001038	17.864256	-0.046158	2.644638
240.585334	2245.038287	17.869261	-0.046168	2.640395
240.584557	2237.079806	17.874266	-0.046163	2.636142
240.501749	2229.099977	17.879271	-0.046142	2.631866
240.398749	2221.095797	17.884275	-0.046118	2.627568
240.465034	2213.138743	17.889280	-0.046125	2.623299
240.339459	2205.177170	17.894285	-0.046097	2.619009
240.116657	2197.224556	17.899290	-0.046050	2.614709
240.218637	2189.234125	17.904295	-0.046064	2.610404
239.899269	2181.295941	17.909299	-0.045999	2.606092
240.297846	2173.296342	17.914304	-0.046068	2.601788
240.225607	2165.328504	17.919309	-0.046049	2.597462
240.096832	2157.285433	17.924314	-0.046020	2.593084
240.146648	2149.206152	17.929319	-0.046024	2.588691
239.927074	2141.274179	17.934323	-0.045978	2.584352
239.989242	2133.363420	17.939328	-0.045985	2.580037
239.919197	2125.419735	17.944333	-0.045966	2.575688
239.690493	2117.469340	17.949338	-0.045919	2.571317
239.785352	2109.477298	17.954343	-0.045931	2.566938
239.540518	2101.546843	17.959347	-0.045880	2.562561
239.520538	2093.618064	17.964352	-0.045871	2.558194
239.848247	2085.603931	17.969357	-0.045927	2.553796
239.680046	2077.635269	17.974362	-0.045891	2.549381
239.418673	2069.699672	17.979367	-0.045837	2.544971
239.413728	2061.741696	17.984371	-0.045831	2.540558
239.476149	2053.773514	17.989376	-0.045837	2.536136
239.465405	2045.773584	17.994381	-0.045830	2.531684
239.509580	2037.793856	17.999386	-0.045833	2.527240
239.454927	2029.853915	18.004391	-0.045818	2.522802
239.184699	2021.925500	18.009395	-0.045762	2.518348
239.224292	2013.952558	18.014400	-0.045764	2.513883
239.305228	2005.926477	18.019405	-0.045774	2.509384
239.301540	1997.953923	18.024410	-0.045768	2.504900
238.916610	1990.072224	18.029415	-0.045692	2.500432
239.027931	1982.055071	18.034419	-0.045707	2.495915
238.939092	1974.129280	18.039424	-0.045685	2.491428
238.868534	1966.137529	18.044429	-0.045667	2.486896
238.925438	1958.188916	18.049434	-0.045672	2.482390
238.995671	1950.219219	18.054439	-0.045680	2.477864
238.826629	1942.266145	18.059443	-0.045644	2.473322
238.854328	1934.270703	18.064448	-0.045644	2.468762
238.742738	1926.310647	18.069453	-0.045618	2.464203
238.612308	1918.373837	18.074458	-0.045588	2.459648
238.718829	1910.410725	18.079463	-0.045603	2.455087
238.657667	1902.436573	18.084467	-0.045586	2.450499
238.737609	1894.462651	18.089472	-0.045596	2.445913
238.537735	1886.538529	18.094477	-0.045554	2.441325
238.257678	1878.611652	18.099482	-0.045496	2.436722
238.421720	1870.569195	18.104487	-0.045522	2.432076
238.284397	1862.573463	18.109491	-0.045491	2.427426
238.330685	1854.633760	18.114496	-0.045494	2.422813
238.233191	1846.680797	18.119501	-0.045471	2.418173
238.162747	1838.731282	18.124506	-0.045453	2.413528
237.970488	1830.787154	18.129511	-0.045412	2.408867
238.043943	1822.802936	18.134515	-0.045420	2.404195
238.147174	1814.859173	18.139520	-0.045434	2.399540
238.026122	1806.937606	18.144525	-0.045407	2.394871
237.902291	1798.949368	18.149530	-0.045378	2.390154
237.913615	1790.983975	18.154535	-0.045375	2.385451
237.871161	1783.024084	18.159539	-0.045362	2.380738
237.757367	1775.102436	18.164544	-0.045336	2.376033
237.820609	1767.101873	18.169549	-0.045342	2.371285
237.752018	1759.161745	18.174554	-0.045324	2.366554
237.926478	1751.204254	18.179559	-0.045352	2.361822
237.586810	1743.287872	18.184563	-0.045283	2.357064
237.607904	1735.308201	18.189568	-0.045282	2.352287
237.502274	1727.329121	18.194573	-0.045257	2.347491
237.494149	1719.374200	18.199578	-0.045250	2.342707
237.616645	1711.427887	18.204583	-0.045268	2.337929
237.406109	1703.481259	18.209587	-0.045224	2.333114
237.327862	1695.530580	18.214592	-0.045204	2.328298
237.415581	1687.542906	18.219597	-0.045215	2.323463
237.242296	1679.626924	18.224602	-0.045178	2.318639
236.960473	1671.718019	18.229607	-0.045120	2.313801
236.925481	1663.714598	18.234611	-0.045108	2.308916
237.026528	1655.743659	18.239616	-0.045122	2.304051
237.030005	1647.804650	18.244621	-0.045117	2.299188
237.103142	1639.836274	18.249626	-0.045126	2.294302
237.149773	1631.873506	18.254631	-0.045129	2.289407
237.159165	1623.921224	18.259635	-0.045126	2.284504
237.049468	1616.019087	18.264640	-0.045100	2.279612
237.075145	1608.062381	18.269645	-0.045100	2.274687
236.780755	1600.053857	18.274650	-0.045040	2.269692
236.832182	1592.097955	18.279655	-0.045044	2.264749
236.809625	1584.149632	18.284659	-0.045035	2.259792
236.772302	1576.220800	18.289664	-0.045023	2.254836
236.641614	1568.275335	18.294669	-0.044993	2.249851
236.650928	1560.315620	18.299674	-0.044990	2.244857
236.566718	1552.406981	18.304679	-0.044969	2.239876
236.464481	1544.469263	18.309683	-0.044945	2.234865
236.283030	1536.513594	18.314688	-0.044906	2.229823
236.366309	1528.544347	18.319693	-0.044916	2.224785
236.342950	1520.600425	18.324698	-0.044907	2.219742
236.155785	1512.690712	18.329703	-0.044867	2.214695
235.989627	1504.722076	18.334707	-0.044831	2.209601
236.129209	1496.766906	18.339712	-0.044851	2.204531
235.858708	1488.871718	18.344717	-0.044796	2.199450
235.893085	1480.906932	18.349722	-0.044797	2.194341
235.870544	1472.916605	18.354727	-0.044788	2.189198
235.768221	1464.973281	18.359731	-0.044763	2.184066
235.643806	1457.069668	18.364736	-0.044735	2.178946
235.729961	1449.101851	18.369741	-0.044746	2.173791
235.805433	1441.132529	18.374746	-0.044755	2.168622
235.521137	1433.248950	18.379751	-0.044697	2.163463
235.318061	1425.319023	18.384755	-0.044654	2.158269
235.471018	1417.360083	18.389760	-0.044677	2.153077
235.371586	1409.399248	18.394765	-0.044653	2.147847
235.238884	1401.467839	18.399770	-0.044624	2.142621
235.181172	1393.555989	18.404775	-0.044608	2.137402
235.064713	1385.602063	18.409779	-0.044581	2.132137
235.137474	1377.658771	18.414784	-0.044589	2.126884
235.062753	1369.726440	18.419789	-0.044570	2.121611
235.177144	1361.782617	18.424794	-0.044586	2.116335
234.947518	1353.826142	18.429799	-0.044538	2.111004
234.649413	1345.890958	18.434803	-0.044478	2.105668
234.895494	1337.934985	18.439808	-0.044518	2.100357
234.690829	1330.032492	18.444813	-0.044475	2.095024
234.667452	1322.071434	18.449818	-0.044465	2.089656
234.735511	1314.138997	18.454823	-0.044473	2.084303
234.817231	1306.203478	18.459827	-0.044483	2.078935
234.721421	1298.300697	18.464832	-0.044460	2.073558
234.345031	1290.389123	18.469837	-0.044385	2.068133
234.471999	1282.422754	18.474842	-0.044403	2.062706
234.557983	1274.511461	18.479847	-0.044414	2.057299
234.393515	1266.576255	18.484851	-0.044378	2.051835
234.433303	1258.637540	18.489856	-0.044381	2.046376
234.492424	1250.699044	18.494861	-0.044386	2.040904
234.579449	1242.782171	18.499866	-0.044397	2.035435
234.518495	1234.823564	18.504871	-0.044381	2.029907
234.330858	1226.913627	18.509875	-0.044341	2.024385
234.240104	1219.026064	18.514880	-0.044319	2.018873
234.027347	1211.107477	18.519885	-0.044274	2.013312
234.329145	1203.108751	18.524890	-0.044325	2.007733
234.229006	1195.222586	18.529895	-0.044301	2.002175
233.924720	1187.346895	18.534899	-0.044239	1.996588
234.016788	1179.388955	18.539904	-0.044251	1.990969
233.839205	1171.480752	18.544909	-0.044213	1.985341
233.791149	1163.564839	18.549914	-0.044199	1.979705
233.705729	1155.665034	18.554919	-0.044178	1.974060
233.662063	1147.714744	18.559923	-0.044165	1.968367
233.697339	1139.799767	18.564928	-0.044166	1.962692
233.549132	1131.904557	18.569933	-0.044133	1.956995
233.573903	1123.929826	18.574938	-0.044133	1.951242
233.565784	1115.995773	18.579943	-0.044126	1.945498
233.486244	1108.085127	18.584947	-0.044106	1.939746
233.494724	1100.184091	18.589952	-0.044103	1.933994
233.356397	1092.258001	18.594957	-0.044072	1.928190
233.197719	1084.375313	18.599962	-0.044037	1.922398
233.147441	1076.465315	18.604967	-0.044022	1.916581
233.222701	1068.504098	18.609971	-0.044031	1.910722
233.436253	1060.567763	18.614976	-0.044066	1.904879
233.177244	1052.720079	18.619981	-0.044013	1.899031
233.016789	1044.821234	18.624986	-0.043978	1.893138
233.218516	1036.873019	18.629991	-0.044010	1.887230
233.013253	1028.991652	18.634995	-0.043967	1.881307
233.016783	1021.097403	18.640000	-0.043962	1.875381
232.878718	1013.186362	18.645005	-0.043931	1.869406
232.676330	1005.284331	18.650010	-0.043888	1.863411
232.813855	997.370669	18.655015	-0.043909	1.857428
232.565405	989.477740	18.660019	-0.043857	1.851396
232.433986	981.583982	18.665024	-0.043828	1.845357
232.371288	973.697037	18.670029	-0.043811	1.839312
232.531804	965.763777	18.675034	-0.043836	1.833238
232.540981	957.850600	18.680039	-0.043832	1.827141
232.316262	949.966580	18.685043	-0.043785	1.821018
232.153177	942.108162	18.690048	-0.043750	1.814902
232.056257	934.207861	18.695053	-0.043727	1.808741
231.948478	926.304284	18.700058	-0.043701	1.802554
231.979933	918.418259	18.705063	-0.043702	1.796377
231.767620	910.477817	18.710067	-0.043657	1.790106
231.832441	902.564965	18.715072	-0.043664	1.783868
231.815397	894.680605	18.720077	-0.043656	1.777621
231.667543	886.789398	18.725082	-0.043623	1.771331
231.727282	878.891421	18.730087	-0.043629	1.765038
231.538708	871.039814	18.735091	-0.043589	1.758729
231.490302	863.163579	18.740096	-0.043575	1.752395
231.501131	855.257469	18.745101	-0.043572	1.746022
231.299590	847.398022	18.750106	-0.043529	1.739636
231.396400	839.514849	18.755111	-0.043542	1.733245
231.386543	831.605685	18.760115	-0.043535	1.726795
231.581322	823.711379	18.765120	-0.043566	1.720360
231.318416	815.884249	18.770125	-0.043512	1.713897
231.150373	807.990268	18.775130	-0.043476	1.707367
231.147920	800.113842	18.780135	-0.043470	1.700847
231.222476	792.226335	18.785139	-0.043479	1.694303
230.856852	784.397680	18.790144	-0.043406	1.687725
230.723159	776.532622	18.795149	-0.043376	1.681122
230.799556	768.658199	18.800154	-0.043385	1.674512
230.710004	760.786244	18.805159	-0.043363	1.667856
230.437936	752.934480	18.810163	-0.043307	1.661166
230.752076	745.039803	18.815168	-0.043361	1.654492
230.834714	737.148731	18.820173	-0.043371	1.647762
230.642551	729.319402	18.825178	-0.043330	1.641020
230.596456	721.479348	18.830183	-0.043316	1.634261
230.365248	713.577923	18.835187	-0.043268	1.627395
230.297278	705.730166	18.840192	-0.043250	1.620569
230.419563	697.858919	18.845197	-0.043268	1.613721
230.349604	689.988240	18.850202	-0.043250	1.606817
230.247498	682.177448	18.855207	-0.043226	1.599931
229.958403	674.362686	18.860211	-0.043167	1.592985
230.247699	666.455264	18.865216	-0.043216	1.586010
230.033048	658.651402	18.870221	-0.043171	1.579023
229.738248	650.842109	18.875226	-0.043111	1.571989
229.726886	642.996251	18.880231	-0.043103	1.564931
229.748136	635.151827	18.885235	-0.043102	1.557848
229.627280	627.316390	18.890240	-0.043075	1.550719
229.532309	619.480896	18.895245	-0.043052	1.543561
229.466449	611.643891	18.900250	-0.043034	1.536373
229.459814	603.809561	18.905255	-0.043028	1.529162
229.241911	595.999315	18.910259	-0.042982	1.521908
229.371050	588.160897	18.915264	-0.043001	1.514645
229.211265	580.347562	18.920269	-0.042967	1.507326
229.065770	572.538397	18.925274	-0.042934	1.499978
229.235034	564.703083	18.930279	-0.042961	1.492618
229.147853	556.872478	18.935283	-0.042939	1.485186
229.029208	549.101438	18.940288	-0.042912	1.477768
228.955115	541.258834	18.945293	-0.042893	1.470251
229.091572	533.403139	18.950298	-0.042914	1.462716
228.763252	525.665017	18.955303	-0.042848	1.455182
228.482761	517.877215	18.960307	-0.042790	1.447569
228.610646	510.067805	18.965312	-0.042809	1.439959
228.593199	502.272500	18.970317	-0.042801	1.432299
228.300575	494.504022	18.975322	-0.042741	1.424580
228.362282	486.709922	18.980327	-0.042747	1.416851
228.332795	478.904013	18.985331	-0.042737	1.409053
228.085991	471.162046	18.990336	-0.042686	1.401240
228.114425	463.379407	18.995341	-0.042686	1.393388
228.229261	455.537049	19.000346	-0.042702	1.385445
228.149842	447.797744	19.005351	-0.042683	1.377529
227.893501	440.048693	19.010355	-0.042630	1.369527
228.113918	432.247016	19.015360	-0.042666	1.361505
227.937917	424.523315	19.020365	-0.042628	1.353448
227.762098	416.770048	19.025370	-0.042590	1.345312
227.586812	409.055259	19.030375	-0.042553	1.337167
227.597897	401.278068	19.035379	-0.042550	1.328939
227.452272	393.562275	19.040384	-0.042517	1.320697
227.594207	385.742986	19.045389	-0.042539	1.312344
227.363096	377.952585	19.050394	-0.042491	1.303901
227.280568	370.248110	19.055399	-0.042470	1.295524
227.121020	362.531974	19.060403	-0.042435	1.287065
227.212147	354.805430	19.065408	-0.042447	1.278585
227.306591	347.078050	19.070413	-0.042460	1.270048
226.915126	339.416596	19.075418	-0.042382	1.261435
226.937740	331.717563	19.080423	-0.042381	1.252800
226.896677	324.004112	19.085427	-0.042369	1.244076
226.783883	316.339089	19.090432	-0.042343	1.235332
226.782193	308.622950	19.095437	-0.042337	1.226488
226.608134	300.961756	19.100442	-0.042300	1.217610
226.764445	293.253137	19.105447	-0.042324	1.208676
226.358107	285.642030	19.110451	-0.042243	1.199679
226.485681	277.958975	19.115456	-0.042262	1.190635
226.303618	270.316782	19.120461	-0.042223	1.181509
226.169789	262.681242	19.125466	-0.042193	1.172329
226.126002	255.042423	19.130471	-0.042180	1.163091
225.988128	247.406236	19.135475	-0.042150	1.153762
225.805755	239.770022	19.140480	-0.042111	1.144349
225.645303	232.165944	19.145485	-0.042076	1.134901
225.671546	224.519061	19.150490	-0.042076	1.125361
225.737675	216.913913	19.155495	-0.042083	1.115800
225.404633	209.349612	19.160499	-0.042016	1.106122
225.204994	201.792656	19.165504	-0.041974	1.096397
225.305289	194.178675	19.170509	-0.041988	1.086578
225.233391	186.622338	19.175514	-0.041969	1.076706
225.005777	179.082461	19.180519	-0.041922	1.066728
224.879572	171.536831	19.185523	-0.041894	1.056672
224.898914	163.975492	19.190528	-0.041892	1.046533
224.579454	156.505154	19.195533	-0.041828	1.036337
224.413336	148.993175	19.200538	-0.041792	1.026020
224.523278	141.467248	19.205543	-0.041808	1.015645
224.231738	134.002965	19.210547	-0.041749	1.005152
224.181559	126.521300	19.215552	-0.041734	0.994583
224.217612	119.002085	19.220557	-0.041736	0.983868
223.989451	111.573715	19.225562	-0.041689	0.973099
223.864779	104.143867	19.230567	-0.041661	0.962235
223.802107	96.717277	19.235571	-0.041644	0.951267
223.602500	89.330545	19.240576	-0.041602	0.940195
223.107183	82.006702	19.245581	-0.041505	0.929008
222.768533	74.671331	19.250586	-0.041438	0.917708
222.921891	67.256119	19.255591	-0.041461	0.906278
222.656296	60.167405	19.260595	-0.041407	0.895101