Fri Mar 12 11:58:15 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.864194	-0.200732	0.000000	-0.000030	0.720534
0.865458	-0.199409	0.005005	-0.000030	0.720537
0.998863	-0.220191	0.010010	-0.000055	0.720543
0.757144	-0.182139	0.015014	-0.000010	0.720533
0.942619	-0.210767	0.020019	-0.000045	0.720542
0.808767	-0.189942	0.025024	-0.000020	0.720536
0.918987	-0.208260	0.030029	-0.000040	0.720538
0.858248	-0.195816	0.035034	-0.000029	0.720542
0.818084	-0.192984	0.040038	-0.000021	0.720533
0.781331	-0.180927	0.045043	-0.000015	0.720544
0.670502	-0.165232	0.050048	0.000006	0.720536
0.750178	-0.179697	0.055053	-0.000009	0.720535
0.849288	-0.193817	0.060058	-0.000027	0.720542
0.826753	-0.193767	0.065062	-0.000023	0.720535
0.716194	-0.203690	0.070067	-0.000002	0.720476
0.708218	-0.332627	0.075072	-0.000001	0.720220
0.701513	-0.328895	0.080077	0.000000	0.720225
0.801774	-0.346907	0.085082	-0.000018	0.720224
0.659827	-0.324440	0.090086	0.000008	0.720219
0.774959	-0.338760	0.095091	-0.000013	0.720231
0.599900	-0.313290	0.100096	0.000019	0.720220
0.670078	-0.400397	0.105101	0.000006	0.720073
0.635472	-0.479999	0.110106	0.000013	0.719904
0.713136	-0.497631	0.115110	-0.000002	0.719896
0.712669	-0.493862	0.120115	-0.000002	0.719904
0.729007	-0.499781	0.125120	-0.000005	0.719898
0.812859	-0.569647	0.130125	-0.000020	0.719789
0.568660	-0.619213	0.135130	0.000025	0.719606
0.660256	-0.640117	0.140134	0.000008	0.719597
0.759984	-0.652769	0.145139	-0.000010	0.719607
0.572543	-0.626275	0.150144	0.000025	0.719593
0.466653	-0.770818	0.155149	0.000044	0.719271
0.741932	-0.817943	0.160154	-0.000007	0.719275
0.691693	-0.813585	0.165158	0.000003	0.719266
0.682097	-0.845512	0.170163	0.000004	0.719200
0.769552	-0.983698	0.175168	-0.000012	0.718958
0.618394	-0.956023	0.180173	0.000016	0.718959
0.600830	-0.949254	0.185178	0.000020	0.718966
0.619170	-1.092094	0.190182	0.000016	0.718691
0.547154	-1.100817	0.195187	0.000030	0.718648
0.643076	-1.120905	0.200192	0.000012	0.718642
0.565294	-1.206679	0.205197	0.000026	0.718446
0.642399	-1.265946	0.210202	0.000012	0.718356
0.414214	-1.229413	0.215206	0.000054	0.718348
0.442293	-1.352572	0.220211	0.000049	0.718114
0.673145	-1.444496	0.225216	0.000006	0.718014
0.810567	-1.468576	0.230221	-0.000019	0.718015
0.469775	-1.562232	0.235226	0.000044	0.717710
0.303339	-1.537838	0.240230	0.000075	0.717699
0.480699	-1.621627	0.245235	0.000042	0.717596
0.603082	-1.752145	0.250240	0.000020	0.717381
0.194116	-1.678667	0.255245	0.000096	0.717382
0.334662	-1.824303	0.260250	0.000070	0.717144
0.222805	-1.837007	0.265254	0.000091	0.717079
0.421947	-1.928657	0.270259	0.000054	0.716968
0.296186	-2.014287	0.275264	0.000077	0.716754
0.282233	-2.018583	0.280269	0.000080	0.716741
0.053392	-2.123109	0.285274	0.000122	0.716453
0.147835	-2.144543	0.290278	0.000105	0.716444
0.214950	-2.271347	0.295283	0.000092	0.716217
-0.140789	-2.251675	0.300288	0.000159	0.716130
-0.613827	-2.226428	0.305293	0.000247	0.716013
-1.215504	-2.182861	0.310298	0.000359	0.715887
-1.444585	-2.146778	0.315302	0.000401	0.715878
-1.545413	-2.276249	0.320307	0.000420	0.715586
-2.189484	-2.182455	0.325312	0.000540	0.715544
-2.643197	-2.112651	0.330317	0.000624	0.715522
-2.845743	-2.220538	0.335322	0.000662	0.715237
-3.105925	-2.179538	0.340326	0.000711	0.715226
-3.293162	-2.142206	0.345331	0.000745	0.715234
-3.518362	-2.246784	0.350336	0.000787	0.714947
-3.950822	-2.190546	0.355341	0.000868	0.714906
-4.013788	-2.176495	0.360346	0.000880	0.714911
-4.266266	-2.190349	0.365350	0.000927	0.714795
-5.036856	-2.145346	0.370355	0.001070	0.714611
-4.847463	-2.181719	0.375360	0.001035	0.714606
-5.155073	-2.127112	0.380365	0.001092	0.714606
-4.909589	-2.232876	0.385370	0.001046	0.714483
-5.997223	-2.146198	0.390374	0.001249	0.714270
-5.796776	-2.177349	0.395379	0.001212	0.714279
-6.265901	-2.096756	0.400384	0.001299	0.714273
-6.117668	-2.123242	0.405389	0.001271	0.714273
-6.129271	-2.243317	0.410394	0.001274	0.714030
-7.608602	-2.013455	0.415398	0.001549	0.713963
-6.926014	-2.128938	0.420403	0.001422	0.713975
-6.597076	-2.193197	0.425408	0.001361	0.713964
-7.255091	-2.073605	0.430413	0.001483	0.713969
-6.985416	-2.227877	0.435418	0.001433	0.713758
-7.874661	-2.126842	0.440422	0.001599	0.713644
-8.071666	-2.086794	0.445427	0.001635	0.713654
-8.062224	-2.091105	0.450432	0.001633	0.713648
-7.857737	-2.127693	0.455437	0.001595	0.713648
-7.474570	-2.226305	0.460442	0.001524	0.713588
-8.659151	-2.132796	0.465446	0.001745	0.713354
-8.361111	-2.182247	0.470451	0.001689	0.713361
-8.514592	-2.158627	0.475456	0.001718	0.713354
-8.653440	-2.134711	0.480461	0.001744	0.713352
-8.621579	-2.135991	0.485466	0.001738	0.713361
-8.815312	-2.204858	0.490470	0.001774	0.713155
-9.958945	-2.067618	0.495475	0.001987	0.713023
-9.671025	-2.122290	0.500480	0.001933	0.713016
-9.752174	-2.107673	0.505485	0.001948	0.713016
-9.610509	-2.130716	0.510490	0.001922	0.713021
-9.817719	-2.096932	0.515494	0.001960	0.713015
-9.564403	-2.164029	0.520499	0.001913	0.712971
-10.396890	-2.149682	0.525504	0.002068	0.712704
-10.527262	-2.124099	0.530509	0.002092	0.712709
-10.608502	-2.110720	0.535514	0.002108	0.712707
-10.349123	-2.159247	0.540518	0.002059	0.712702
-10.486884	-2.131446	0.545523	0.002085	0.712708
-10.890335	-2.061597	0.550528	0.002160	0.712704
-10.709295	-2.187262	0.555533	0.002126	0.712518
-11.433568	-2.125692	0.560538	0.002261	0.712384
-11.712512	-2.081042	0.565542	0.002313	0.712374
-11.363930	-2.138489	0.570547	0.002248	0.712383
-11.370294	-2.138294	0.575552	0.002249	0.712381
-11.715870	-2.079695	0.580557	0.002314	0.712375
-11.485870	-2.116913	0.585562	0.002271	0.712383
-11.704645	-2.175408	0.590566	0.002312	0.712189
-12.275385	-2.124475	0.595571	0.002418	0.712088
-12.357992	-2.111673	0.600576	0.002433	0.712084
-12.311163	-2.119193	0.605581	0.002425	0.712085
-11.962788	-2.179348	0.610586	0.002360	0.712089
-12.464842	-2.094705	0.615590	0.002453	0.712080
-12.341659	-2.113402	0.620595	0.002430	0.712086
-12.726771	-2.210027	0.625600	0.002502	0.711757
-13.428362	-2.087006	0.630605	0.002633	0.711753
-13.520326	-2.065371	0.635610	0.002650	0.711763
-13.212202	-2.125364	0.640614	0.002592	0.711753
-13.246511	-2.114629	0.645619	0.002599	0.711762
-13.541638	-2.064466	0.650624	0.002654	0.711757
-13.397357	-2.092092	0.655629	0.002627	0.711754
-13.227768	-2.230970	0.660634	0.002595	0.711537
-14.561480	-2.038274	0.665638	0.002844	0.711447
-14.278357	-2.084732	0.670643	0.002791	0.711455
-14.093238	-2.120222	0.675648	0.002756	0.711450
-14.379878	-2.069730	0.680653	0.002810	0.711449
-14.135811	-2.108367	0.685658	0.002764	0.711459
-14.098421	-2.121446	0.690662	0.002757	0.711446
-14.171715	-2.212339	0.695667	0.002771	0.711239
-15.519006	-2.023691	0.700672	0.003022	0.711136
-15.489768	-2.031912	0.705677	0.003016	0.711130
-14.808678	-2.148742	0.710682	0.002890	0.711139
-15.499521	-2.031227	0.715686	0.003018	0.711128
-15.230788	-2.074889	0.720691	0.002968	0.711136
-14.956604	-2.123355	0.725696	0.002917	0.711137
-15.332955	-2.090237	0.730701	0.002987	0.711069
-15.838877	-2.098347	0.735706	0.003082	0.710873
-15.740728	-2.122013	0.740710	0.003063	0.710861
-15.653134	-2.132695	0.745715	0.003047	0.710871
-15.975473	-2.077519	0.750720	0.003107	0.710866
-15.902433	-2.091589	0.755725	0.003093	0.710864
-15.665201	-2.131986	0.760730	0.003049	0.710868
-16.142715	-2.145129	0.765734	0.003138	0.710672
-17.226055	-2.023239	0.770739	0.003340	0.710529
-16.595083	-2.137165	0.775744	0.003222	0.710527
-16.675409	-2.124686	0.780749	0.003237	0.710523
-16.944238	-2.071228	0.785754	0.003287	0.710534
-16.866049	-2.091374	0.790758	0.003273	0.710522
-16.747762	-2.107059	0.795763	0.003251	0.710532
-17.066411	-2.115292	0.800768	0.003310	0.710402
-18.121695	-2.024228	0.805773	0.003507	0.710209
-17.314633	-2.164694	0.810778	0.003356	0.710215
-17.777532	-2.087043	0.815782	0.003443	0.710206
-17.893945	-2.062116	0.820787	0.003464	0.710214
-17.416050	-2.148686	0.825792	0.003375	0.710211
-17.817066	-2.077454	0.830797	0.003450	0.710211
-18.001570	-2.095111	0.835802	0.003484	0.710110
-18.806100	-2.064813	0.840806	0.003634	0.709884
-18.301250	-2.152714	0.845811	0.003540	0.709888
-18.872444	-2.051542	0.850816	0.003646	0.709887
-19.019362	-2.025358	0.855821	0.003674	0.709887
-18.331633	-2.144210	0.860826	0.003546	0.709894
-18.706939	-2.082516	0.865830	0.003616	0.709884
-18.992698	-2.029246	0.870835	0.003669	0.709888
-19.024883	-2.160476	0.875840	0.003675	0.709614
-19.310200	-2.125938	0.880845	0.003728	0.709582
-19.387394	-2.107223	0.885850	0.003742	0.709592
-19.754520	-2.046125	0.890854	0.003811	0.709583
-19.481987	-2.091923	0.895859	0.003760	0.709589
-19.469408	-2.094202	0.900864	0.003758	0.709588
-19.696511	-2.054390	0.905869	0.003800	0.709587
-20.016437	-2.156122	0.910874	0.003859	0.709270
-20.473055	-2.082308	0.915878	0.003944	0.709254
-20.713513	-2.037736	0.920883	0.003989	0.709258
-20.197352	-2.129296	0.925888	0.003893	0.709259
-20.320494	-2.109064	0.930893	0.003916	0.709255
-20.353651	-2.099214	0.935898	0.003922	0.709263
-20.466692	-2.084020	0.940902	0.003943	0.709253
-20.456415	-2.223820	0.945907	0.003941	0.708977
-21.003794	-2.138894	0.950912	0.004043	0.708952
-21.514096	-2.050010	0.955917	0.004138	0.708948
-20.906000	-2.153319	0.960922	0.004025	0.708958
-21.104829	-2.121818	0.965926	0.004062	0.708950
-21.622938	-2.026436	0.970931	0.004159	0.708956
-21.597529	-2.044296	0.975936	0.004154	0.708929
-21.963267	-2.127340	0.980941	0.004222	0.708633
-22.004224	-2.116609	0.985946	0.004230	0.708639
-22.430750	-2.043628	0.990950	0.004309	0.708633
-22.259734	-2.072041	0.995955	0.004277	0.708637
-22.145613	-2.094172	1.000960	0.004256	0.708634
-22.734360	-1.990096	1.005965	0.004365	0.708632
-22.090582	-2.102574	1.010970	0.004246	0.708637
-22.278470	-2.169221	1.015974	0.004281	0.708436
-23.342080	-2.025382	1.020979	0.004479	0.708344
-22.928509	-2.100028	1.025984	0.004402	0.708343
-22.835436	-2.117199	1.030989	0.004384	0.708341
-23.021349	-2.080050	1.035994	0.004419	0.708349
-23.157897	-2.061086	1.040998	0.004444	0.708339
-22.848110	-2.112287	1.046003	0.004387	0.708347
-23.184820	-2.198974	1.051008	0.004450	0.708053
-24.262591	-2.031597	1.056013	0.004650	0.708003
-23.976721	-2.077682	1.061018	0.004597	0.708013
-23.740915	-2.123447	1.066022	0.004553	0.708005
-23.887570	-2.094659	1.071027	0.004580	0.708011
-24.184328	-2.044489	1.076032	0.004636	0.708005
-24.040985	-2.070659	1.081037	0.004609	0.708004
-24.076943	-2.174799	1.086042	0.004616	0.707782
-25.460449	-1.974279	1.091046	0.004873	0.707690
-25.062176	-2.043787	1.096051	0.004799	0.707693
-24.606301	-2.124029	1.101056	0.004714	0.707695
-25.054361	-2.045838	1.106061	0.004798	0.707692
-24.885225	-2.075750	1.111066	0.004766	0.707692
-24.799986	-2.094794	1.116070	0.004750	0.707684
-24.915006	-2.140128	1.121075	0.004772	0.707552
-25.901846	-2.055801	1.126080	0.004955	0.707369
-25.587112	-2.113455	1.131085	0.004897	0.707365
-25.726487	-2.084682	1.136090	0.004923	0.707373
-26.210385	-2.003990	1.141094	0.005013	0.707362
-25.850782	-2.064741	1.146099	0.004946	0.707369
-25.444590	-2.137997	1.151104	0.004870	0.707367
-25.942590	-2.090845	1.156109	0.004963	0.707284
-26.807995	-2.040954	1.161114	0.005124	0.707074
-26.470563	-2.104987	1.166118	0.005061	0.707066
-26.674479	-2.065800	1.171123	0.005099	0.707072
-26.797968	-2.044448	1.176128	0.005122	0.707071
-26.849775	-2.037544	1.181133	0.005132	0.707066
-26.389327	-2.115224	1.186138	0.005046	0.707075
-26.664156	-2.076498	1.191142	0.005097	0.707054
-27.255964	-2.124344	1.196147	0.005208	0.706746
-27.103847	-2.152740	1.201152	0.005179	0.706744
-27.674194	-2.053948	1.206157	0.005285	0.706738
-27.239412	-2.126785	1.211162	0.005204	0.706747
-27.358278	-2.109869	1.216166	0.005227	0.706739
-27.437660	-2.092959	1.221171	0.005241	0.706744
-27.502638	-2.143156	1.226176	0.005254	0.706620
-28.765233	-2.010897	1.231181	0.005489	0.706434
-27.996548	-2.143801	1.236186	0.005345	0.706442
-28.505891	-2.057667	1.241190	0.005440	0.706433
-28.477106	-2.060699	1.246195	0.005435	0.706437
-28.006112	-2.145199	1.251200	0.005347	0.706436
-28.382680	-2.079353	1.256205	0.005417	0.706433
-28.443728	-2.127621	1.261210	0.005429	0.706314
-29.265043	-2.079955	1.266214	0.005582	0.706116
-29.076953	-2.111852	1.271219	0.005547	0.706119
-29.527819	-2.030974	1.276224	0.005631	0.706120
-29.426553	-2.051781	1.281229	0.005612	0.706115
-28.754737	-2.167772	1.286234	0.005487	0.706122
-29.303060	-2.073093	1.291238	0.005589	0.706116
-29.284424	-2.134178	1.296243	0.005585	0.706000
-29.959045	-2.085488	1.301248	0.005711	0.705856
-29.861014	-2.104631	1.306253	0.005693	0.705853
-29.939283	-2.085592	1.311258	0.005707	0.705863
-30.169244	-2.050069	1.316262	0.005750	0.705852
-29.900195	-2.096788	1.321267	0.005700	0.705854
-30.097516	-2.059166	1.326272	0.005737	0.705859
-30.361790	-2.131874	1.331277	0.005786	0.705618
-30.792405	-2.099719	1.336282	0.005866	0.705528
-30.925553	-2.081722	1.341286	0.005891	0.705517
-30.794146	-2.102587	1.346291	0.005866	0.705522
-30.666413	-2.126131	1.351296	0.005843	0.705520
-30.779632	-2.108623	1.356301	0.005864	0.705515
-30.779255	-2.118502	1.361306	0.005864	0.705495
-31.640704	-2.110935	1.366310	0.006024	0.705201
-31.374596	-2.155582	1.371315	0.005975	0.705207
-31.737086	-2.090260	1.376320	0.006042	0.705208
-31.877698	-2.067634	1.381325	0.006068	0.705204
-31.465743	-2.135994	1.386330	0.005991	0.705214
-31.692832	-2.101130	1.391334	0.006034	0.705202
-31.994828	-2.097341	1.396339	0.006090	0.705102
-32.698009	-2.079420	1.401344	0.006221	0.704885
-32.359703	-2.143528	1.406349	0.006158	0.704878
-32.519007	-2.109624	1.411354	0.006188	0.704889
-32.655464	-2.091496	1.416358	0.006213	0.704876
-32.455126	-2.122366	1.421363	0.006176	0.704886
-32.745794	-2.072056	1.426368	0.006230	0.704883
-32.900694	-2.099774	1.431373	0.006259	0.704772
-33.201187	-2.136042	1.436378	0.006315	0.704591
-33.268999	-2.128715	1.441382	0.006327	0.704581
-33.830829	-2.026847	1.446387	0.006432	0.704584
-33.306071	-2.121522	1.451392	0.006334	0.704582
-33.412500	-2.104406	1.456397	0.006354	0.704578
-33.593544	-2.068138	1.461402	0.006388	0.704586
-33.659655	-2.125835	1.466406	0.006400	0.704446
-34.360739	-2.096137	1.471411	0.006531	0.704254
-33.942879	-2.170130	1.476416	0.006453	0.704255
-34.716683	-2.034959	1.481421	0.006597	0.704250
-34.263843	-2.111510	1.486426	0.006513	0.704258
-34.116850	-2.143678	1.491430	0.006485	0.704246
-34.548529	-2.063734	1.496435	0.006565	0.704252
-34.303927	-2.181475	1.501440	0.006520	0.704103
-35.273338	-2.091852	1.506445	0.006700	0.703935
-35.134999	-2.109549	1.511450	0.006675	0.703949
-35.510319	-2.048205	1.516454	0.006745	0.703938
-35.415197	-2.063266	1.521459	0.006727	0.703941
-35.051187	-2.127273	1.526464	0.006659	0.703943
-35.581282	-2.033923	1.531469	0.006758	0.703941
-35.155953	-2.170543	1.536474	0.006679	0.703818
-36.187425	-2.082504	1.541478	0.006871	0.703625
-36.303045	-2.060302	1.546483	0.006892	0.703628
-36.332111	-2.056124	1.551488	0.006898	0.703626
-36.186000	-2.083488	1.556493	0.006870	0.703623
-35.975529	-2.117492	1.561498	0.006831	0.703631
-36.226153	-2.075514	1.566502	0.006878	0.703625
-35.941873	-2.173616	1.571507	0.006825	0.703529
-36.780563	-2.119827	1.576512	0.006981	0.703336
-37.237166	-2.042862	1.581517	0.007066	0.703327
-37.130581	-2.056489	1.586522	0.007046	0.703338
-36.764804	-2.124797	1.591526	0.006978	0.703332
-37.054060	-2.072565	1.596531	0.007032	0.703333
-37.216616	-2.041725	1.601536	0.007062	0.703337
-37.097655	-2.111337	1.606541	0.007040	0.703239
-37.765019	-2.109730	1.611546	0.007164	0.703002
-37.966235	-2.076364	1.616550	0.007202	0.702997
-38.134693	-2.043196	1.621555	0.007233	0.703003
-37.688278	-2.122752	1.626560	0.007150	0.703003
-38.094260	-2.052992	1.631565	0.007226	0.702998
-37.833373	-2.096453	1.636570	0.007177	0.703004
-38.007469	-2.092538	1.641574	0.007210	0.702949
-38.664695	-2.104737	1.646579	0.007332	0.702688
-38.658389	-2.105512	1.651584	0.007331	0.702689
-38.938644	-2.057626	1.656589	0.007383	0.702685
-38.617642	-2.110418	1.661594	0.007323	0.702694
-38.832105	-2.076233	1.666598	0.007363	0.702685
-38.824415	-2.078529	1.671603	0.007362	0.702683
-38.551036	-2.168406	1.676608	0.007311	0.702600
-39.833543	-2.060204	1.681613	0.007550	0.702357
-39.657564	-2.086137	1.686618	0.007517	0.702368
-39.816849	-2.062405	1.691622	0.007547	0.702358
-39.851013	-2.055000	1.696627	0.007553	0.702361
-39.894431	-2.045635	1.701632	0.007561	0.702364
-39.906235	-2.047273	1.706637	0.007563	0.702357
-39.582781	-2.099927	1.711642	0.007503	0.702367
-40.170597	-2.125428	1.716646	0.007612	0.702103
-40.878841	-2.016582	1.721651	0.007744	0.702068
-40.438614	-2.094692	1.726656	0.007662	0.702069
-40.518101	-2.083295	1.731661	0.007677	0.702063
-40.473944	-2.085340	1.736666	0.007669	0.702075
-40.552256	-2.078823	1.741670	0.007683	0.702060
-40.586207	-2.070298	1.746675	0.007690	0.702065
-41.104653	-2.117018	1.751680	0.007786	0.701783
-41.644053	-2.045713	1.756685	0.007887	0.701733
-41.186698	-2.122019	1.761690	0.007802	0.701744
-41.243635	-2.116223	1.766694	0.007812	0.701735
-41.475599	-2.074203	1.771699	0.007855	0.701736
-41.053216	-2.148631	1.776704	0.007777	0.701738
-41.529820	-2.082235	1.781709	0.007866	0.701700
-42.456082	-2.048754	1.786714	0.008038	0.701434
-42.261231	-2.085002	1.791718	0.008002	0.701431
-42.359597	-2.067267	1.796723	0.008020	0.701431
-42.451825	-2.048815	1.801728	0.008037	0.701435
-42.481245	-2.047576	1.806733	0.008043	0.701427
-42.090720	-2.112278	1.811738	0.007970	0.701437
-42.143755	-2.107021	1.816742	0.007980	0.701429
-42.940693	-2.114581	1.821747	0.008128	0.701126
-43.030846	-2.101432	1.826752	0.008145	0.701120
-43.241368	-2.067281	1.831757	0.008184	0.701113
-43.094591	-2.089522	1.836762	0.008157	0.701121
-43.219538	-2.070130	1.841766	0.008180	0.701115
-43.425213	-2.032489	1.846771	0.008218	0.701117
-43.152573	-2.080488	1.851776	0.008168	0.701118
-43.680177	-2.107383	1.856781	0.008266	0.700873
-43.746804	-2.096040	1.861786	0.008278	0.700872
-44.079059	-2.040949	1.866790	0.008340	0.700864
-44.048406	-2.046221	1.871795	0.008334	0.700864
-43.750832	-2.095972	1.876800	0.008279	0.700871
-44.112801	-2.033695	1.881805	0.008346	0.700866
-43.885281	-2.124918	1.886810	0.008304	0.700763
-44.601934	-2.113991	1.891814	0.008438	0.700526
-44.305462	-2.165242	1.896819	0.008382	0.700530
-44.497536	-2.128678	1.901824	0.008418	0.700534
-45.006234	-2.042543	1.906829	0.008513	0.700525
-44.490512	-2.132084	1.911834	0.008417	0.700530
-44.914716	-2.058321	1.916838	0.008496	0.700526
-45.464072	-2.107396	1.921843	0.008598	0.700228
-45.237746	-2.153221	1.926848	0.008556	0.700217
-45.657747	-2.082437	1.931853	0.008634	0.700209
-45.537852	-2.100045	1.936858	0.008612	0.700216
-45.575674	-2.096455	1.941862	0.008619	0.700210
-45.693632	-2.073339	1.946867	0.008641	0.700214
-45.620368	-2.130657	1.951872	0.008627	0.700124
-46.691358	-2.056537	1.956877	0.008827	0.699887
-46.290144	-2.125048	1.961882	0.008752	0.699893
-46.458821	-2.098543	1.966886	0.008783	0.699886
-46.771265	-2.041128	1.971891	0.008842	0.699890
-46.259988	-2.131191	1.976896	0.008746	0.699892
-46.421257	-2.106545	1.981901	0.008776	0.699884
-46.626584	-2.133041	1.986906	0.008815	0.699755
-47.522251	-2.054057	1.991910	0.008981	0.699592
-47.393412	-2.076533	1.996915	0.008957	0.699593
-47.528305	-2.052404	2.001920	0.008982	0.699593
-47.251940	-2.101611	2.011917	0.008931	0.699593
-47.460103	-2.064792	2.021914	0.008970	0.699592
-47.319313	-2.141211	2.031910	0.008944	0.699488
-48.228015	-2.092177	2.041907	0.009113	0.699259
-48.249359	-2.046577	2.051904	0.009117	0.699343
-47.663911	-2.112500	2.061901	0.009008	0.699422
-47.519886	-2.084642	2.071898	0.008981	0.699530
-47.337104	-2.084707	2.081894	0.008947	0.699596
-47.405709	-2.073701	2.091891	0.008960	0.699594
-47.179298	-2.116463	2.101888	0.008918	0.699589
-47.231969	-2.104988	2.111885	0.008927	0.699593
-47.600646	-2.037810	2.121882	0.008996	0.699596
-47.361062	-2.082075	2.131878	0.008951	0.699593
-47.328886	-2.089042	2.141875	0.008945	0.699590
-47.232513	-2.038271	2.151872	0.008927	0.699728
-46.326356	-2.120386	2.161869	0.008759	0.699890
-46.842369	-2.027473	2.171866	0.008855	0.699891
-46.399204	-2.109699	2.181862	0.008772	0.699885
-46.610244	-2.056769	2.191859	0.008812	0.699916
-45.646650	-2.083256	2.201856	0.008632	0.700211
-45.591236	-2.092827	2.211853	0.008622	0.700211
-45.720903	-2.070239	2.221850	0.008646	0.700210
-45.733387	-2.058531	2.231846	0.008648	0.700230
-45.046376	-2.036162	2.241843	0.008520	0.700523
-44.730757	-2.092212	2.251840	0.008462	0.700524
-44.715863	-2.093130	2.261837	0.008459	0.700527
-44.933935	-2.000070	2.271834	0.008499	0.700637
-43.698187	-2.106747	2.281830	0.008269	0.700868
-43.893861	-2.072429	2.291827	0.008306	0.700866
-43.980001	-2.055985	2.301824	0.008322	0.700869
-43.514185	-2.070770	2.311821	0.008235	0.701007
-43.352827	-2.046877	2.321818	0.008205	0.701114
-43.325933	-2.051091	2.331814	0.008200	0.701115
-43.385817	-1.996574	2.341811	0.008211	0.701204
-42.223725	-2.092753	2.351808	0.007995	0.701428
-42.386510	-2.062448	2.361805	0.008025	0.701431
-42.342461	-2.069451	2.371802	0.008017	0.701433
-41.744472	-2.043141	2.381798	0.007906	0.701702
-41.789597	-2.017674	2.391795	0.007914	0.701737
-41.278269	-2.109235	2.401792	0.007819	0.701736
-41.319487	-2.023318	2.411789	0.007827	0.701895
-40.681538	-2.050990	2.421786	0.007708	0.702069
-40.773942	-2.034201	2.431782	0.007725	0.702070
-40.665767	-2.040001	2.441779	0.007705	0.702097
-39.799155	-2.062844	2.451776	0.007543	0.702363
-39.753430	-2.069989	2.461773	0.007535	0.702365
-39.710054	-2.078571	2.471770	0.007527	0.702364
-39.391393	-2.031113	2.481766	0.007468	0.702575
-39.160755	-2.018827	2.491763	0.007425	0.702682
-38.827252	-2.077051	2.501760	0.007363	0.702685
-38.818544	-2.042631	2.511757	0.007361	0.702758
-37.843005	-2.097180	2.521754	0.007179	0.702999
-37.879535	-2.091592	2.531750	0.007186	0.702997
-38.011685	-2.067833	2.541747	0.007211	0.702997
-37.681591	-2.034427	2.551744	0.007149	0.703184
-37.036851	-2.074168	2.561741	0.007029	0.703335
-36.957227	-2.089058	2.571738	0.007014	0.703334
-37.048640	-2.074305	2.581734	0.007031	0.703331
-36.358880	-2.056880	2.591731	0.006903	0.703614
-36.202278	-2.080305	2.601728	0.006874	0.703623
-36.207594	-2.076217	2.611725	0.006875	0.703630
-35.971618	-2.043219	2.621722	0.006831	0.703781
-35.236519	-2.093418	2.631718	0.006694	0.703944
-35.339394	-2.076353	2.641715	0.006713	0.703942
-35.356878	-2.072186	2.651712	0.006716	0.703944
-34.704967	-2.044546	2.661709	0.006595	0.704234
-34.191874	-2.126017	2.671706	0.006500	0.704254
-34.387279	-2.091797	2.681702	0.006536	0.704253
-34.503495	-2.022575	2.691699	0.006557	0.704351
-33.621157	-2.065054	2.701696	0.006393	0.704582
-33.813725	-2.029479	2.711693	0.006429	0.704584
-33.680737	-2.038059	2.721690	0.006404	0.704615
-33.051709	-2.019267	2.731686	0.006287	0.704879
-32.523634	-2.114998	2.741683	0.006189	0.704875
-32.762720	-2.071983	2.751680	0.006233	0.704876
-32.322721	-2.053441	2.761677	0.006151	0.705072
-31.610593	-2.115179	2.771674	0.006019	0.705203
-32.038848	-2.039063	2.781670	0.006099	0.705202
-31.630586	-2.111569	2.791667	0.006023	0.705203
-31.190844	-2.034641	2.801664	0.005941	0.705516
-30.999671	-2.067785	2.811661	0.005905	0.705517
-31.054280	-2.058707	2.821658	0.005915	0.705516
-30.686879	-2.015590	2.831654	0.005847	0.705735
-29.903931	-2.096371	2.841651	0.005701	0.705853
-30.112159	-2.057733	2.851648	0.005740	0.705856
-29.811037	-2.110904	2.861645	0.005684	0.705857
-29.348325	-2.066994	2.871642	0.005598	0.706111
-29.528946	-2.030750	2.881638	0.005631	0.706119
-29.146430	-2.100451	2.891635	0.005560	0.706116
-28.909833	-2.051997	2.901632	0.005516	0.706298
-28.125843	-2.121320	2.911629	0.005370	0.706440
-28.405733	-2.072669	2.921626	0.005422	0.706437
-28.369686	-2.072714	2.931622	0.005415	0.706450
-27.614740	-2.059887	2.941619	0.005275	0.706746
-27.524843	-2.075597	2.951616	0.005258	0.706747
-27.476565	-2.083266	2.961613	0.005249	0.706749
-27.069193	-2.051505	2.971610	0.005173	0.706958
-26.643849	-2.069204	2.981606	0.005094	0.707075
-26.556154	-2.086273	2.991603	0.005078	0.707072
-26.768039	-2.022263	3.001600	0.005117	0.707125
-25.660812	-2.094548	3.011597	0.004911	0.707376
-25.687571	-2.090749	3.021594	0.004916	0.707374
-25.843265	-2.064786	3.031590	0.004945	0.707370
-25.371526	-2.033257	3.041587	0.004857	0.707602
-25.072020	-2.040508	3.051584	0.004801	0.707695
-24.809680	-2.086368	3.061581	0.004753	0.707697
-24.921449	-2.015435	3.071578	0.004773	0.707799
-23.976727	-2.079985	3.081574	0.004598	0.708007
-24.075953	-2.061634	3.091571	0.004616	0.708008
-24.186095	-2.042545	3.101568	0.004637	0.708007
-23.136839	-2.076984	3.111565	0.004441	0.708313
-23.138615	-2.059231	3.121562	0.004441	0.708348
-23.048865	-2.077057	3.131558	0.004425	0.708344
-23.306787	-1.983109	3.141555	0.004473	0.708440
-22.058644	-2.109514	3.151552	0.004240	0.708633
-22.275441	-2.070520	3.161549	0.004281	0.708634
-22.507253	-2.028811	3.171546	0.004324	0.708634
-21.728246	-2.027192	3.181542	0.004179	0.708916
-21.438140	-2.062030	3.191539	0.004125	0.708949
-21.466564	-2.058366	3.201536	0.004130	0.708947
-21.128985	-2.046069	3.211533	0.004067	0.709092
-20.493551	-2.074967	3.221530	0.003949	0.709260
-20.630573	-2.053043	3.231526	0.003975	0.709255
-20.982303	-1.971256	3.241523	0.004040	0.709294
-19.758288	-2.042044	3.251520	0.003812	0.709588
-19.553404	-2.076327	3.261517	0.003774	0.709593
-19.788796	-2.035702	3.271514	0.003818	0.709590
-19.203303	-2.048911	3.281510	0.003709	0.709772
-19.097995	-2.011195	3.291507	0.003689	0.709885
-18.686649	-2.082349	3.301504	0.003613	0.709890
-18.738090	-2.058480	3.311501	0.003622	0.709919
-18.021740	-2.037594	3.321498	0.003489	0.710216
-17.793145	-2.079658	3.331494	0.003446	0.710213
-17.930314	-2.057009	3.341491	0.003472	0.710210
-17.493267	-2.064487	3.351488	0.003390	0.710350
-16.655659	-2.122713	3.361485	0.003234	0.710532
-16.977369	-2.065457	3.371482	0.003294	0.710532
-16.692388	-2.117139	3.381478	0.003241	0.710530
-16.463332	-2.051902	3.391475	0.003199	0.710742
-15.897557	-2.091618	3.401472	0.003093	0.710864
-15.809035	-2.105393	3.411469	0.003077	0.710868
-15.756239	-2.113741	3.421466	0.003067	0.710870
-15.264684	-2.093112	3.431462	0.002975	0.711086
-15.488515	-2.031135	3.441459	0.003017	0.711130
-14.933998	-2.129202	3.451456	0.002914	0.711132
-15.018047	-2.053318	3.461453	0.002930	0.711253
-14.045015	-2.127473	3.471450	0.002748	0.711451
-14.029146	-2.130063	3.481446	0.002745	0.711452
-14.341485	-2.075617	3.491443	0.002804	0.711449
-13.501515	-2.119093	3.501440	0.002647	0.711661
-13.362694	-2.095968	3.511437	0.002621	0.711756
-13.168995	-2.129344	3.521434	0.002585	0.711759
-13.316128	-2.091442	3.531430	0.002613	0.711782
-12.709045	-2.048228	3.541427	0.002500	0.712084
-12.206382	-2.139126	3.551424	0.002406	0.712081
-12.584630	-2.068783	3.561421	0.002476	0.712087
-11.885510	-2.100354	3.571418	0.002346	0.712272
-11.867862	-2.047669	3.581414	0.002343	0.712383
-11.637600	-2.089715	3.591411	0.002300	0.712381
-11.657209	-2.045647	3.601408	0.002304	0.712462
-10.862618	-2.063872	3.611405	0.002156	0.712708
-10.473213	-2.133213	3.621402	0.002083	0.712708
-10.715265	-2.090984	3.631398	0.002128	0.712706
-10.291154	-2.049121	3.641395	0.002049	0.712940
-9.852503	-2.086277	3.651392	0.001968	0.713021
-9.905131	-2.075601	3.661389	0.001978	0.713024
-9.597877	-2.089379	3.671386	0.001920	0.713106
-8.893052	-2.089405	3.681382	0.001789	0.713355
-8.775343	-2.109706	3.691379	0.001767	0.713357
-8.762602	-2.112995	3.701376	0.001765	0.713355
-8.464497	-2.093251	3.711373	0.001709	0.713499
-7.738407	-2.146246	3.721370	0.001574	0.713651
-8.051316	-2.091436	3.731366	0.001632	0.713649
-7.871072	-2.125984	3.741363	0.001599	0.713645
-7.492331	-2.056326	3.751360	0.001528	0.713917
-6.813820	-2.151411	3.761357	0.001402	0.713968
-6.929320	-2.132050	3.771354	0.001424	0.713966
-6.995835	-2.092627	3.781350	0.001436	0.714021
-6.257897	-2.098060	3.791347	0.001299	0.714271
-6.040466	-2.136243	3.801344	0.001258	0.714272
-6.266685	-2.095465	3.811341	0.001300	0.714273
-5.583009	-2.103068	3.821338	0.001173	0.714500
-5.451018	-2.073483	3.831334	0.001148	0.714605
-4.938127	-2.165956	3.841331	0.001053	0.714603
-5.270308	-2.106301	3.851328	0.001115	0.714604
-4.457214	-2.099689	3.861325	0.000963	0.714905
-4.393976	-2.112251	3.871322	0.000952	0.714902
-4.408069	-2.110131	3.881318	0.000954	0.714901
-4.232718	-2.057594	3.891315	0.000921	0.715068
-3.490630	-2.109624	3.901312	0.000783	0.715227
-3.479185	-2.111306	3.911309	0.000781	0.715227
-3.394937	-2.125681	3.921306	0.000766	0.715229
-3.074380	-2.027594	3.931302	0.000706	0.715536
-2.553830	-2.118628	3.941299	0.000609	0.715540
-2.774146	-2.081033	3.951296	0.000650	0.715537
-2.735582	-1.977081	3.961293	0.000643	0.715756
-1.755595	-2.089427	3.971290	0.000460	0.715880
-2.128223	-2.022216	3.981286	0.000530	0.715881
-1.595546	-2.068277	3.991283	0.000430	0.715978
-1.447422	-2.019988	4.001280	0.000403	0.716126
-2.066128	-1.909100	4.011277	0.000518	0.716127
-1.242737	-1.962853	4.021274	0.000365	0.716311
-1.612196	-1.830737	4.031270	0.000433	0.716443
-1.159530	-1.893252	4.041267	0.000349	0.716478
-0.859060	-1.809703	4.051264	0.000293	0.716750
-0.887866	-1.803305	4.061261	0.000299	0.716752
-0.960552	-1.667296	4.071258	0.000312	0.716996
-1.027420	-1.613353	4.081254	0.000324	0.717079
-0.940584	-1.513803	4.091251	0.000308	0.717306
-0.684975	-1.525897	4.101248	0.000261	0.717373
-0.452226	-1.413822	4.111245	0.000217	0.717676
-0.496273	-1.372207	4.121242	0.000225	0.717743
-0.579605	-1.220406	4.131238	0.000241	0.718013
-0.510055	-1.144254	4.141235	0.000228	0.718188
-0.637950	-1.030025	4.151232	0.000252	0.718369
-0.287817	-0.955268	4.161229	0.000186	0.718640
-0.277982	-0.857987	4.171226	0.000184	0.718835
-0.350376	-0.740450	4.181222	0.000198	0.719042
-0.225471	-0.648947	4.191219	0.000174	0.719266
-0.199513	-0.489641	4.201216	0.000170	0.719589
-0.252630	-0.364720	4.211213	0.000179	0.719817
-0.368583	-0.209730	4.221210	0.000201	0.720081
-0.163860	-0.104338	4.231206	0.000163	0.720361
0.152997	-0.015921	4.241203	0.000104	0.720646
0.000000	0.176757	4.251200	0.000132	0.720972
0.024311	0.770878	4.256205	0.000127	0.722148
0.242664	2.007498	4.261210	0.000086	0.724649
0.360907	3.835399	4.266214	0.000062	0.728260
0.805150	6.172223	4.271219	-0.000022	0.732950
1.079689	9.046167	4.276224	-0.000075	0.738585
1.211467	12.413899	4.281229	-0.000102	0.745070
1.535511	16.217120	4.286234	-0.000164	0.752384
1.740347	20.426139	4.291238	-0.000205	0.760346
2.310500	24.980686	4.296243	-0.000314	0.768983
2.605673	29.953470	4.301248	-0.000373	0.778197
3.180870	35.215632	4.306253	-0.000483	0.787914
3.703010	40.820621	4.311258	-0.000584	0.798105
4.015463	46.749934	4.316262	-0.000646	0.808671
4.696236	52.910049	4.321267	-0.000777	0.819613
5.047694	59.401018	4.326272	-0.000846	0.830876
5.148333	66.143572	4.331277	-0.000870	0.842337
7.633471	72.706042	4.336282	-0.001337	0.854044
10.115645	79.516382	4.341286	-0.001803	0.865996
10.811473	86.849475	4.346291	-0.001938	0.878120
11.449883	94.361699	4.351296	-0.002061	0.890349
12.263898	101.991751	4.356301	-0.002218	0.902645
13.681046	109.683890	4.361306	-0.002487	0.915035
14.719906	117.549176	4.366310	-0.002685	0.927422
15.488552	125.601257	4.371315	-0.002834	0.939856
16.258860	133.748188	4.376320	-0.002982	0.952269
17.104250	141.962158	4.381325	-0.003145	0.964639
17.922465	150.282152	4.386330	-0.003303	0.977000
19.300505	158.585446	4.391334	-0.003565	0.989321
20.320258	167.010810	4.396339	-0.003760	1.001574
21.293490	175.472684	4.401344	-0.003947	1.013718
21.688044	184.055912	4.406349	-0.004026	1.025747
22.475057	192.621643	4.411354	-0.004178	1.037706
23.088827	201.224332	4.416358	-0.004298	1.049537
24.119802	209.791123	4.421363	-0.004496	1.061284
25.537661	218.332880	4.426368	-0.004765	1.072957
26.410076	226.958934	4.431373	-0.004933	1.084491
27.571075	235.569452	4.436378	-0.005155	1.095947
28.265709	244.243140	4.441382	-0.005290	1.107262
29.036681	252.920866	4.446387	-0.005439	1.118484
29.768592	261.593404	4.451392	-0.005581	1.129580
30.511817	270.260609	4.456397	-0.005725	1.140562
31.755564	278.875606	4.461402	-0.005962	1.151481
32.032527	287.607655	4.466406	-0.006020	1.162238
32.791828	296.238324	4.471411	-0.006167	1.172873
33.748355	304.828216	4.476416	-0.006350	1.183403
34.453718	313.450275	4.481421	-0.006487	1.193828
35.346560	322.018803	4.486426	-0.006659	1.204136
35.856840	330.643920	4.491430	-0.006760	1.214347
36.955652	339.158559	4.496435	-0.006970	1.224460
37.570962	347.781305	4.501440	-0.007090	1.234519
38.238627	356.318543	4.506445	-0.007220	1.244410
39.139723	364.838993	4.511450	-0.007393	1.254248
40.171554	373.308233	4.516454	-0.007591	1.263976
40.862873	381.845605	4.521459	-0.007725	1.273642
41.488972	390.360393	4.526464	-0.007847	1.283197
42.511059	398.798053	4.531469	-0.008043	1.292670
43.172534	407.303788	4.536474	-0.008172	1.302081
43.777487	415.866568	4.541478	-0.008290	1.311476
44.668153	424.340107	4.546483	-0.008462	1.320760
45.253413	432.787902	4.551488	-0.008576	1.329896
46.133129	441.171487	4.556493	-0.008745	1.338954
47.121921	449.540257	4.561498	-0.008935	1.347955
47.321331	458.027687	4.566502	-0.008978	1.356881
47.812380	466.425797	4.571507	-0.009074	1.365707
48.592535	474.794335	4.576512	-0.009225	1.374495
49.260911	483.155674	4.581517	-0.009355	1.383201
49.871149	491.554680	4.586522	-0.009474	1.391880
50.493110	499.900551	4.591526	-0.009595	1.400454
51.058880	508.255559	4.596531	-0.009706	1.408975
52.015336	516.559949	4.601536	-0.009890	1.417458
52.679026	524.873568	4.606541	-0.010019	1.425852
53.280807	533.240937	4.611546	-0.010136	1.434239
53.910569	541.546629	4.616550	-0.010259	1.442521
54.740294	549.831167	4.621555	-0.010419	1.450767
55.639590	558.120947	4.626560	-0.010592	1.458983
56.032497	566.457339	4.631565	-0.010670	1.467116
56.367830	574.870046	4.636570	-0.010738	1.475269
56.777720	583.159542	4.641574	-0.010820	1.483271
57.219719	591.455477	4.646579	-0.010908	1.491241
57.997135	599.710419	4.651584	-0.011058	1.499182
58.609149	607.951988	4.656589	-0.011177	1.507042
59.457901	616.210205	4.661594	-0.011340	1.514913
59.858827	624.484890	4.666598	-0.011420	1.522691
60.385729	632.745035	4.671603	-0.011524	1.530434
61.021454	641.004808	4.676608	-0.011648	1.538154
61.433730	649.258150	4.681613	-0.011730	1.545796
61.974310	657.546677	4.686618	-0.011836	1.553452
62.437860	665.772621	4.691622	-0.011928	1.561002
62.916490	674.002512	4.696627	-0.012022	1.568520
63.326244	682.270958	4.701632	-0.012104	1.576028
64.115841	690.441884	4.706637	-0.012256	1.583467
65.108158	698.618532	4.711642	-0.012446	1.590905
65.687793	706.848154	4.716646	-0.012559	1.598297
66.319864	715.044109	4.721651	-0.012682	1.605632
67.033005	723.264432	4.726656	-0.012821	1.612966
67.437161	731.491261	4.731661	-0.012901	1.620229
68.194200	739.690277	4.736666	-0.013048	1.627485
68.578256	747.993582	4.741670	-0.013124	1.634747
69.122873	756.179437	4.746675	-0.013231	1.641897
69.408981	764.411011	4.751680	-0.013290	1.649020
69.625123	772.638194	4.756685	-0.013335	1.656099
70.174688	780.826958	4.761690	-0.013443	1.663160
70.910996	788.979721	4.766694	-0.013586	1.670186
71.268853	797.195117	4.771699	-0.013658	1.677184
71.784426	805.372748	4.776704	-0.013759	1.684143
72.364063	813.534201	4.781709	-0.013872	1.691067
73.013397	821.708455	4.786714	-0.013998	1.697983
73.360879	829.884687	4.791718	-0.014068	1.704833
74.136601	838.037862	4.796723	-0.014218	1.711691
74.492141	846.247131	4.801728	-0.014290	1.718514
74.601605	854.438136	4.806733	-0.014315	1.725264
75.000632	862.635202	4.811738	-0.014395	1.732028
75.537847	870.778107	4.816742	-0.014500	1.738740
76.395398	878.869991	4.821747	-0.014665	1.745426
76.800098	887.083545	4.826752	-0.014746	1.752126
77.250458	895.236333	4.831757	-0.014835	1.758758
77.465124	903.430472	4.836762	-0.014880	1.765368
78.034361	911.574938	4.841766	-0.014992	1.771959
78.411974	919.750520	4.846771	-0.015067	1.778525
78.727242	927.916413	4.851776	-0.015131	1.785052
79.126428	936.101685	4.856781	-0.015211	1.791580
79.684614	944.258093	4.861786	-0.015320	1.798082
80.178276	952.372397	4.866790	-0.015418	1.804519
80.531697	960.522881	4.871795	-0.015489	1.810944
81.133534	968.646289	4.876800	-0.015606	1.817355
81.464576	976.789053	4.881805	-0.015673	1.823726
82.069949	984.922021	4.886810	-0.015791	1.830100
82.225367	993.103121	4.891814	-0.015825	1.836436
82.833949	1001.194880	4.896819	-0.015944	1.842734
83.445924	1009.331524	4.901824	-0.016063	1.849045
83.575358	1017.514838	4.906829	-0.016093	1.855314
83.830047	1025.677662	4.911834	-0.016145	1.861561
84.476027	1033.767589	4.916838	-0.016271	1.867777
84.753519	1041.955369	4.921843	-0.016328	1.874004
85.337273	1050.037515	4.926848	-0.016442	1.880165
85.775978	1058.138636	4.931853	-0.016529	1.886304
86.057328	1066.311361	4.936858	-0.016586	1.892458
86.431765	1074.434436	4.941862	-0.016661	1.898566
87.011039	1082.508857	4.946867	-0.016775	1.904641
87.723572	1090.624399	4.951872	-0.016913	1.910742
88.179817	1098.749901	4.956877	-0.017003	1.916802
88.581520	1106.863334	4.961882	-0.017083	1.922828
89.212501	1114.968438	4.966886	-0.017206	1.928854
89.484415	1123.131143	4.971891	-0.017262	1.934864
89.711341	1131.291789	4.976896	-0.017309	1.940849
90.047764	1139.411145	4.981901	-0.017377	1.946797
90.538269	1147.570437	4.986906	-0.017474	1.952773
90.807586	1155.687630	4.991910	-0.017529	1.958676
91.180808	1163.771972	4.996915	-0.017604	1.964549
91.748454	1171.858525	5.001920	-0.017715	1.970426
92.160306	1179.954172	5.006925	-0.017797	1.976276
92.780774	1188.031490	5.011930	-0.017918	1.982117
93.129736	1196.151664	5.016934	-0.017988	1.987943
93.619608	1204.265345	5.021939	-0.018084	1.993762
94.035551	1212.378623	5.026944	-0.018167	1.999556
94.404557	1220.466347	5.031949	-0.018241	2.005310
94.880956	1228.595223	5.036954	-0.018335	2.011087
95.099825	1236.739469	5.041958	-0.018381	2.016832
95.444731	1244.826497	5.046963	-0.018451	2.022534
96.080543	1252.919251	5.051968	-0.018574	2.028253
96.286791	1261.095061	5.056973	-0.018618	2.033970
96.542514	1269.188902	5.061978	-0.018671	2.039619
97.162090	1277.230753	5.066982	-0.018792	2.045253
97.638041	1285.323150	5.071987	-0.018885	2.050892
97.838750	1293.466742	5.076992	-0.018928	2.056523
98.279062	1301.529984	5.081997	-0.019015	2.062107
99.033002	1309.581492	5.087002	-0.019161	2.067700
99.209652	1317.740555	5.092006	-0.019199	2.073293
99.593966	1325.824120	5.097011	-0.019276	2.078840
100.065042	1333.913522	5.102016	-0.019369	2.084385
100.310496	1342.006907	5.107021	-0.019420	2.089895
101.008197	1350.089760	5.112026	-0.019555	2.095428
101.579760	1358.151621	5.117030	-0.019667	2.100920
102.046578	1366.244850	5.122035	-0.019759	2.106409
102.344234	1374.424092	5.127040	-0.019820	2.111924
102.435020	1382.564171	5.132045	-0.019842	2.117379
102.771142	1390.629068	5.137050	-0.019910	2.122793
103.081989	1398.710715	5.142054	-0.019973	2.128201
103.334100	1406.818322	5.147059	-0.020025	2.133608
104.070294	1414.848424	5.152064	-0.020168	2.138996
104.297635	1422.935370	5.157069	-0.020215	2.144359
104.613778	1431.034784	5.162074	-0.020279	2.149725
104.846206	1439.156193	5.167078	-0.020328	2.155085
105.517138	1447.173670	5.172083	-0.020458	2.160404
105.833511	1455.278216	5.177088	-0.020522	2.165734
106.165522	1463.361222	5.182093	-0.020589	2.171038
106.371142	1471.490149	5.187098	-0.020633	2.176347
106.716720	1479.553502	5.192102	-0.020702	2.181613
107.028829	1487.634114	5.197107	-0.020766	2.186875
107.359160	1495.762818	5.202112	-0.020833	2.192157
107.789985	1503.821277	5.207117	-0.020918	2.197390
108.155229	1511.881552	5.212122	-0.020991	2.202606
108.481606	1519.955729	5.217126	-0.021057	2.207814
108.681492	1528.078022	5.222131	-0.021100	2.213030
109.301871	1536.118904	5.227136	-0.021221	2.218219
109.882396	1544.148602	5.232141	-0.021334	2.223385
110.472720	1552.218907	5.237146	-0.021449	2.228566
110.903719	1560.332463	5.242150	-0.021535	2.233747
111.167756	1568.406735	5.247155	-0.021589	2.238877
111.598177	1576.479721	5.252160	-0.021675	2.244010
111.766135	1584.573594	5.257165	-0.021711	2.249120
112.003441	1592.697254	5.262170	-0.021761	2.254244
112.307104	1600.769261	5.267174	-0.021822	2.259329
112.754864	1608.817185	5.272179	-0.021911	2.264400
113.137889	1616.913494	5.277184	-0.021988	2.269484
113.033458	1625.117309	5.282189	-0.021973	2.274582
113.597233	1633.114002	5.287194	-0.022084	2.279597
114.140514	1641.108844	5.292198	-0.022190	2.284598
114.348655	1649.200644	5.297203	-0.022234	2.289620
114.791144	1657.283681	5.302208	-0.022322	2.294645
114.915840	1665.353809	5.307213	-0.022350	2.299624
115.246738	1673.419839	5.312218	-0.022417	2.304607
115.509489	1681.503985	5.317222	-0.022471	2.309584
115.886861	1689.581647	5.322227	-0.022547	2.314557
116.395867	1697.616204	5.327232	-0.022647	2.319503
116.436530	1705.694469	5.332237	-0.022660	2.324426
116.911392	1713.746160	5.337242	-0.022753	2.329359
117.287446	1721.842872	5.342246	-0.022829	2.334301
117.670970	1729.875172	5.347251	-0.022905	2.339193
118.082112	1737.936079	5.352256	-0.022987	2.344095
118.656004	1745.987691	5.357261	-0.023099	2.348994
119.228550	1754.090735	5.362266	-0.023211	2.353913
119.691878	1762.136830	5.367270	-0.023303	2.358779
120.059186	1770.198727	5.372275	-0.023376	2.363637
120.447565	1778.273582	5.377280	-0.023454	2.368494
120.520720	1786.387508	5.382285	-0.023473	2.373339
120.942226	1794.443722	5.387290	-0.023556	2.378168
120.862496	1802.555148	5.392294	-0.023547	2.382979
121.108576	1810.608192	5.397299	-0.023598	2.387773
121.371769	1818.704885	5.402304	-0.023652	2.392583
121.762765	1826.743033	5.407309	-0.023730	2.397360
122.262596	1834.779258	5.412314	-0.023829	2.402134
122.611140	1842.831490	5.417318	-0.023899	2.406897
123.241398	1850.853142	5.422323	-0.024021	2.411653
123.578478	1858.943577	5.427328	-0.024089	2.416418
123.707915	1867.006630	5.432333	-0.024119	2.421141
124.634263	1875.003089	5.437338	-0.024296	2.425878
124.994920	1883.112553	5.442342	-0.024369	2.430628
125.203600	1891.256027	5.447347	-0.024413	2.435376
125.521404	1899.300136	5.452352	-0.024477	2.440066
125.671182	1907.344791	5.457357	-0.024510	2.444734
125.883796	1915.415876	5.462362	-0.024555	2.449413
126.206406	1923.486489	5.467366	-0.024621	2.454091
126.496296	1931.515379	5.472371	-0.024680	2.458734
126.954989	1939.557149	5.477376	-0.024771	2.463388
127.133365	1947.631142	5.482381	-0.024809	2.468031
127.694960	1955.678140	5.487386	-0.024919	2.472678
128.117929	1963.735443	5.492390	-0.025003	2.477312
128.286358	1971.784745	5.497395	-0.025039	2.481914
128.612848	1979.843137	5.502400	-0.025105	2.486524
128.835559	1987.930152	5.507405	-0.025152	2.491134
129.060721	1996.023988	5.512410	-0.025199	2.495739
129.454641	2004.042651	5.517414	-0.025278	2.500306
129.739500	2012.082834	5.522419	-0.025336	2.504868
130.491372	2020.100426	5.527424	-0.025481	2.509444
130.547772	2028.237023	5.532429	-0.025497	2.514027
130.856440	2036.290201	5.537434	-0.025560	2.518573
131.250654	2044.307042	5.542438	-0.025639	2.523097
131.378240	2052.374897	5.547443	-0.025668	2.527622
131.610228	2060.468559	5.552448	-0.025716	2.532161
131.780760	2068.519193	5.557453	-0.025753	2.536664
132.140953	2076.570736	5.562458	-0.025825	2.541172
132.234275	2084.626353	5.567462	-0.025848	2.545656
132.578137	2092.687780	5.572467	-0.025917	2.550152
132.923187	2100.761814	5.577472	-0.025987	2.554648
133.107703	2108.788103	5.582477	-0.026026	2.559098
133.560953	2116.813183	5.587482	-0.026116	2.563559
134.010635	2124.858365	5.592486	-0.026205	2.568022
134.297299	2132.917927	5.597491	-0.026264	2.572474
134.687136	2140.984339	5.602496	-0.026341	2.576929
134.991476	2149.020113	5.607501	-0.026403	2.581354
135.269640	2157.075723	5.612506	-0.026460	2.585780
135.510841	2165.164249	5.617510	-0.026511	2.590214
135.747374	2173.422692	5.622515	-0.026560	2.594733
136.026010	2181.392173	5.627520	-0.026617	2.599090
136.246757	2189.377818	5.632525	-0.026663	2.603443
136.553235	2197.393948	5.637530	-0.026726	2.607812
136.852604	2205.446811	5.642534	-0.026787	2.612193
137.075805	2213.490758	5.647539	-0.026833	2.616557
137.438269	2221.518280	5.652544	-0.026906	2.620914
137.666221	2229.541233	5.657549	-0.026954	2.625252
137.851379	2237.601185	5.662554	-0.026994	2.629600
138.067272	2245.690006	5.667558	-0.027039	2.633958
138.433311	2253.706558	5.672563	-0.027112	2.638280
138.811551	2261.721555	5.677568	-0.027188	2.642595
138.970112	2269.779482	5.682573	-0.027223	2.646911
139.058085	2277.869858	5.687578	-0.027245	2.651233
139.461985	2285.922812	5.692582	-0.027325	2.655549
139.811466	2293.924664	5.697587	-0.027395	2.659826
140.284329	2301.971056	5.702592	-0.027489	2.664129
140.530037	2310.021857	5.707597	-0.027540	2.668412
140.895111	2318.097212	5.712602	-0.027613	2.672709
140.941281	2326.192561	5.717606	-0.027627	2.676989
141.205758	2334.202772	5.722611	-0.027681	2.681231
141.656915	2342.226974	5.727616	-0.027770	2.685485
141.928364	2350.254982	5.732621	-0.027826	2.689724
141.964951	2358.356284	5.737626	-0.027838	2.693979
142.423255	2366.374341	5.742630	-0.027929	2.698211
142.565158	2374.405085	5.747635	-0.027960	2.702422
142.632282	2382.490311	5.752640	-0.027978	2.706651
142.961093	2390.525728	5.757645	-0.028045	2.710864
143.491734	2398.565294	5.762650	-0.028149	2.715084
143.686000	2406.624215	5.767654	-0.028190	2.719287
143.707103	2414.647175	5.772659	-0.028199	2.723455
144.301143	2422.668477	5.777664	-0.028315	2.727650
144.590888	2430.738642	5.782669	-0.028374	2.731845
144.804866	2438.824334	5.787674	-0.028419	2.736038
144.903861	2446.887137	5.792678	-0.028443	2.740204
145.320589	2454.874982	5.797683	-0.028526	2.744346
145.736674	2462.942015	5.802688	-0.028609	2.748522
146.105124	2471.029609	5.807693	-0.028683	2.752698
146.533941	2479.092755	5.812698	-0.028768	2.756860
146.975450	2487.096690	5.817702	-0.028855	2.760986
147.185104	2495.096669	5.822707	-0.028899	2.765089
147.670208	2503.118625	5.827712	-0.028995	2.769214
147.799103	2511.198140	5.832717	-0.029024	2.773341
147.760977	2519.275507	5.837722	-0.029022	2.777451
148.188060	2527.291575	5.842726	-0.029107	2.781551
148.278401	2535.323182	5.847731	-0.029129	2.785633
148.667737	2543.356569	5.852736	-0.029207	2.789728
148.901223	2551.418817	5.857741	-0.029256	2.793822
149.300994	2559.442255	5.862746	-0.029335	2.797900
149.543909	2567.493894	5.867750	-0.029386	2.801977
149.548967	2575.535230	5.872755	-0.029392	2.806029
149.840798	2583.570707	5.877760	-0.029451	2.810089
150.056149	2591.646044	5.882765	-0.029497	2.814158
150.415827	2599.661211	5.887770	-0.029569	2.818200
150.807102	2607.690709	5.892774	-0.029647	2.822245
151.096724	2615.724839	5.897779	-0.029706	2.826280
151.518894	2623.778631	5.902784	-0.029790	2.830327
151.710632	2631.886112	5.907789	-0.029831	2.834382
151.920481	2639.894115	5.912794	-0.029875	2.838383
152.286860	2647.910837	5.917798	-0.029949	2.842391
152.470120	2655.932796	5.922803	-0.029988	2.846385
152.847300	2663.988909	5.927808	-0.030064	2.850402
153.160337	2672.039878	5.932813	-0.030127	2.854407
153.414908	2680.062182	5.937818	-0.030180	2.858389
153.679396	2688.114314	5.942822	-0.030234	2.862380
153.965984	2696.128476	5.947827	-0.030293	2.866349
154.390483	2704.160637	5.952832	-0.030377	2.870328
154.850252	2712.224374	5.957837	-0.030468	2.874319
155.374324	2720.235772	5.962842	-0.030571	2.878283
155.896097	2728.249209	5.967846	-0.030673	2.882241
155.853906	2736.327860	5.972851	-0.030671	2.886196
156.433209	2744.356754	5.977856	-0.030784	2.890154
156.748792	2752.428818	5.982861	-0.030848	2.894114
156.992997	2760.467503	5.987866	-0.030898	2.898048
157.275405	2768.527135	5.992870	-0.030956	2.901989
157.794905	2776.512610	5.997875	-0.031058	2.905901
158.104148	2784.588268	6.002880	-0.031121	2.909840
158.236497	2792.736373	6.007885	-0.031151	2.913800
158.693914	2800.730951	6.012890	-0.031241	2.917697
158.903803	2808.757157	6.017894	-0.031286	2.921591
158.999001	2816.763422	6.022899	-0.031309	2.925464
159.397922	2824.767887	6.027904	-0.031388	2.929347
159.643211	2832.818754	6.032909	-0.031439	2.933239
159.714963	2840.899347	6.037914	-0.031458	2.937132
159.990610	2848.921739	6.042918	-0.031514	2.941001
160.303783	2856.911725	6.047923	-0.031578	2.944852
160.706451	2864.953492	6.052928	-0.031658	2.948728
161.011580	2872.999634	6.057933	-0.031720	2.952595
161.287477	2881.051808	6.062938	-0.031777	2.956458
161.537779	2889.077509	6.067942	-0.031828	2.960303
161.826248	2897.078228	6.072947	-0.031887	2.964132
162.284156	2905.142128	6.077952	-0.031978	2.967996
162.709508	2913.177571	6.082957	-0.032062	2.971838
162.791799	2921.263618	6.087962	-0.032083	2.975683
163.150494	2929.271394	6.092966	-0.032155	2.979499
163.375344	2937.304553	6.097971	-0.032202	2.983316
163.806744	2945.348612	6.102976	-0.032288	2.987143
163.936727	2953.412735	6.107981	-0.032317	2.990960
164.089799	2961.478168	6.112986	-0.032351	2.994773
164.710510	2969.442867	6.117990	-0.032472	2.998558
164.790336	2977.488329	6.122995	-0.032492	3.002348
164.978474	2985.535255	6.128000	-0.032532	3.006140
165.306834	2993.542433	6.133005	-0.032598	3.009916
165.682671	3001.600165	6.138010	-0.032674	3.013713
166.079299	3009.616052	6.143014	-0.032753	3.017486
166.325042	3017.660638	6.148019	-0.032804	3.021260
166.792685	3025.652799	6.153024	-0.032896	3.025016
166.784124	3033.730203	6.158029	-0.032900	3.028784
167.176701	3041.784670	6.163034	-0.032978	3.032556
167.676296	3049.828199	6.168038	-0.033076	3.036324
167.934236	3057.816284	6.173043	-0.033129	3.040049
168.099211	3065.871700	6.178048	-0.033165	3.043796
168.330613	3073.900634	6.183053	-0.033214	3.047530
168.741965	3081.950011	6.188058	-0.033296	3.051277
169.090363	3090.025433	6.193062	-0.033366	3.055028
169.440426	3098.010707	6.198067	-0.033436	3.058733
169.826105	3106.044861	6.203072	-0.033513	3.062458
169.932180	3114.101994	6.208077	-0.033538	3.066176
170.181076	3122.132674	6.213082	-0.033590	3.069884
170.804498	3130.243792	6.218086	-0.033711	3.073641
171.054081	3138.246665	6.223091	-0.033763	3.077327
171.295640	3146.277794	6.228096	-0.033813	3.081021
171.700170	3154.229210	6.233101	-0.033893	3.084682
172.035427	3162.256695	6.238106	-0.033961	3.088369
172.194338	3170.356865	6.243110	-0.033996	3.092078
172.341511	3178.393416	6.248115	-0.034029	3.095752
172.844218	3186.375090	6.253120	-0.034127	3.099413
173.005808	3194.398614	6.258125	-0.034163	3.103073
173.197254	3202.473365	6.263130	-0.034204	3.106754
173.511977	3210.499400	6.268134	-0.034267	3.110413
173.611238	3218.557224	6.273139	-0.034291	3.114073
173.746379	3226.588612	6.278144	-0.034322	3.117719
174.071674	3234.603000	6.283149	-0.034387	3.121360
174.286658	3242.614358	6.288154	-0.034433	3.124992
174.541715	3250.674079	6.293158	-0.034485	3.128642
174.827949	3258.688324	6.298163	-0.034544	3.132269
175.153888	3266.735836	6.303168	-0.034610	3.135909
175.363260	3274.775172	6.308173	-0.034654	3.139536
175.669522	3282.785910	6.313178	-0.034716	3.143149
175.919687	3290.839357	6.318182	-0.034768	3.146775
176.167036	3298.848161	6.323187	-0.034819	3.150377
176.460284	3306.939206	6.328192	-0.034879	3.154014
176.875752	3314.946843	6.333197	-0.034962	3.157614
177.101514	3322.970381	6.338202	-0.035009	3.161209
177.406113	3330.947236	6.343206	-0.035071	3.164783
177.810991	3338.971208	6.348211	-0.035152	3.168377
177.972619	3347.077099	6.353216	-0.035187	3.171994
178.107480	3355.109930	6.358221	-0.035217	3.175572
178.008188	3363.155435	6.363226	-0.035204	3.179143
178.537666	3371.153109	6.368230	-0.035308	3.182715
178.850276	3379.165308	6.373235	-0.035371	3.186280
179.037894	3387.226105	6.378240	-0.035412	3.189857
179.173641	3395.274868	6.383245	-0.035442	3.193423
179.549637	3403.298516	6.388250	-0.035517	3.196983
179.886873	3411.310918	6.393254	-0.035585	3.200533
179.775799	3419.301908	6.398259	-0.035570	3.204051
180.374702	3427.355763	6.403264	-0.035687	3.207622
180.941305	3435.379337	6.408269	-0.035797	3.211175
180.833382	3443.439381	6.413274	-0.035782	3.214711
181.188200	3451.476843	6.418278	-0.035854	3.218253
181.629635	3459.471746	6.423283	-0.035941	3.221776
181.940966	3467.482813	6.428288	-0.036004	3.225297
182.106768	3475.544960	6.433293	-0.036040	3.228830
182.090940	3483.636538	6.438298	-0.036043	3.232365
182.557386	3491.704978	6.443302	-0.036135	3.235905
182.893954	3499.649817	6.448307	-0.036203	3.239382
183.191699	3507.683710	6.453312	-0.036263	3.242893
183.516958	3515.716019	6.458317	-0.036329	3.246400
183.702856	3523.703188	6.463322	-0.036369	3.249879
184.112902	3531.743857	6.468326	-0.036451	3.253385
184.399180	3539.783169	6.473331	-0.036509	3.256883
184.652128	3547.812690	6.478336	-0.036562	3.260370
184.850131	3555.829255	6.483341	-0.036604	3.263847
185.098597	3563.862872	6.488346	-0.036655	3.267329
185.502599	3571.927916	6.493350	-0.036736	3.270827
185.717580	3579.936413	6.498355	-0.036781	3.274289
186.071302	3587.972815	6.503360	-0.036852	3.277765
186.500000	3595.987914	6.508365	-0.036937	3.281231
186.511327	3604.000719	6.513370	-0.036944	3.284676
186.772626	3612.061973	6.518374	-0.036998	3.288148
187.032839	3620.081737	6.523379	-0.037052	3.291599
187.184141	3628.143876	6.528384	-0.037085	3.295059
187.222057	3636.168539	6.533389	-0.037098	3.298496
187.540329	3644.164861	6.538394	-0.037162	3.301928
187.688340	3652.208970	6.543398	-0.037195	3.305370
187.923421	3660.238426	6.548403	-0.037244	3.308805
188.013270	3668.317083	6.553408	-0.037266	3.312253
188.177924	3676.363107	6.558413	-0.037302	3.315685
188.565663	3684.321477	6.563418	-0.037379	3.319085
188.967855	3692.342053	6.568422	-0.037459	3.322509
189.048380	3700.344956	6.573427	-0.037479	3.325909
189.365838	3708.397900	6.578432	-0.037544	3.329336
189.705320	3716.430829	6.583437	-0.037612	3.332752
190.033447	3724.470948	6.588442	-0.037679	3.336167
190.652974	3732.437169	6.593446	-0.037799	3.339558
190.758419	3740.468351	6.598451	-0.037824	3.342954
190.889680	3748.552898	6.603456	-0.037854	3.346369
191.296969	3756.561838	6.608461	-0.037935	3.349760
191.551242	3764.613089	6.613466	-0.037987	3.353159
191.711470	3772.692630	6.618470	-0.038022	3.356563
191.689209	3780.668298	6.623475	-0.038024	3.359914
191.995024	3788.687011	6.628480	-0.038086	3.363291
192.225994	3796.738223	6.633485	-0.038134	3.366676
192.328805	3804.740008	6.638490	-0.038158	3.370031
192.573982	3812.819041	6.643494	-0.038209	3.373421
192.691346	3820.861909	6.648499	-0.038236	3.376788
192.833271	3828.867406	6.653504	-0.038268	3.380137
193.261399	3836.869411	6.658509	-0.038353	3.383491
193.579760	3844.873850	6.663514	-0.038417	3.386838
193.832822	3852.912123	6.668518	-0.038470	3.390195
193.980616	3861.037169	6.673523	-0.038503	3.393580
194.122959	3869.050606	6.678528	-0.038534	3.396915
194.319429	3877.018560	6.683533	-0.038576	3.400230
194.454911	3885.012284	6.688538	-0.038606	3.403550
195.020498	3893.048914	6.693542	-0.038717	3.406900
195.333205	3901.029478	6.698547	-0.038780	3.410214
195.571413	3909.104954	6.703552	-0.038830	3.413562
195.625149	3917.160641	6.708557	-0.038845	3.416892
195.672133	3925.161963	6.713562	-0.038859	3.420196
195.948822	3933.182440	6.718566	-0.038916	3.423512
196.198642	3941.196357	6.723571	-0.038968	3.426822
196.487461	3949.239237	6.728576	-0.039027	3.430142
196.775231	3957.271145	6.733581	-0.039086	3.433453
197.086558	3965.286974	6.738586	-0.039149	3.436756
197.343170	3973.328820	6.743590	-0.039202	3.440065
197.607175	3981.339075	6.748595	-0.039256	3.443357
197.797683	3989.360027	6.753600	-0.039297	3.446648
198.066309	3997.352659	6.758605	-0.039352	3.449927
198.104057	4005.440403	6.763610	-0.039364	3.453234
198.474162	4013.477851	6.768614	-0.039439	3.456529
198.529509	4021.496323	6.773619	-0.039454	3.459802
198.915200	4029.496763	6.778624	-0.039531	3.463075
199.079794	4037.560188	6.783629	-0.039567	3.466364
199.405527	4045.531767	6.788634	-0.039633	3.469617
199.760775	4053.652359	6.793638	-0.039704	3.472929
200.070867	4061.669061	6.798643	-0.039767	3.476194
200.141316	4069.635384	6.803648	-0.039786	3.479428
200.435197	4077.661684	6.808653	-0.039846	3.482690
200.773407	4085.646652	6.813658	-0.039914	3.485934
201.057682	4093.719123	6.818662	-0.039972	3.489208
201.184445	4101.737440	6.823667	-0.040001	3.492453
201.431492	4109.776328	6.828672	-0.040052	3.495706
201.633750	4117.789917	6.833677	-0.040095	3.498945
201.990045	4125.775820	6.838682	-0.040166	3.502174
202.309097	4133.822576	6.843686	-0.040231	3.505424
202.388679	4141.840321	6.848691	-0.040251	3.508651
202.686530	4149.885203	6.853696	-0.040312	3.511894
202.964661	4157.935290	6.858701	-0.040369	3.515134
203.263528	4165.914261	6.863706	-0.040430	3.518344
203.171740	4173.982757	6.868710	-0.040418	3.521575
203.321184	4181.958315	6.873715	-0.040451	3.524773
203.675984	4189.997402	6.878720	-0.040522	3.527999
203.690961	4198.052614	6.883725	-0.040530	3.531219
203.834061	4206.092977	6.888730	-0.040562	3.534434
204.277848	4214.119598	6.893734	-0.040650	3.537649
204.390609	4222.133989	6.898739	-0.040676	3.540847
204.594493	4230.143348	6.903744	-0.040719	3.544042
204.944416	4238.194632	6.908749	-0.040790	3.547255
205.213585	4246.215412	6.913754	-0.040845	3.550451
205.724205	4254.342752	6.918758	-0.040945	3.553694
205.667946	4262.357713	6.923763	-0.040940	3.556872
206.036584	4270.297896	6.928768	-0.041014	3.560030
206.183964	4278.312926	6.933773	-0.041047	3.563209
206.278002	4286.339911	6.938778	-0.041069	3.566388
206.785612	4294.327887	6.943782	-0.041169	3.569560
206.794698	4302.374802	6.948787	-0.041176	3.572739
206.987995	4310.414625	6.953792	-0.041217	3.575917
207.232897	4318.430204	6.958797	-0.041268	3.579084
207.442978	4326.427782	6.963802	-0.041312	3.582241
207.742056	4334.477643	6.968806	-0.041373	3.585417
207.909341	4342.483162	6.973811	-0.041410	3.588570
208.134780	4350.535332	6.978816	-0.041457	3.591740
208.505697	4358.542874	6.983821	-0.041531	3.594893
208.477095	4366.552854	6.988826	-0.041531	3.598033
208.773083	4374.598400	6.993830	-0.041591	3.601194
208.750010	4382.574207	6.998835	-0.041592	3.604316
208.997543	4390.597546	7.003840	-0.041644	3.607461
209.212396	4398.639117	7.008845	-0.041689	3.610610
209.521330	4406.672351	7.013850	-0.041752	3.613755
209.690354	4414.727414	7.018854	-0.041788	3.616902
209.988976	4422.697910	7.023859	-0.041849	3.620016
210.570994	4430.706838	7.028864	-0.041963	3.623151
210.984554	4438.758051	7.033869	-0.042045	3.626295
211.375135	4446.742525	7.038874	-0.042123	3.629410
211.730667	4454.853084	7.043878	-0.042194	3.632569
212.008229	4462.890168	7.048883	-0.042251	3.635696
212.186322	4470.872719	7.053888	-0.042290	3.638796
212.413989	4478.920820	7.058893	-0.042337	3.641919
212.695400	4486.883477	7.063898	-0.042395	3.645009
213.168144	4494.930337	7.068902	-0.042488	3.648134
213.203662	4502.962522	7.073907	-0.042500	3.651238
213.288125	4511.019258	7.078912	-0.042521	3.654351
213.559305	4519.064528	7.083917	-0.042577	3.657461
213.521556	4527.064002	7.088922	-0.042575	3.660543
214.069011	4535.086557	7.093926	-0.042682	3.663647
214.458349	4543.052156	7.098931	-0.042760	3.666722
214.711113	4551.100437	7.103936	-0.042812	3.669822
214.728147	4559.177969	7.108941	-0.042821	3.672925
214.959226	4567.175590	7.113946	-0.042869	3.676000
215.234194	4575.182792	7.118950	-0.042925	3.679078
215.265262	4583.206532	7.123955	-0.042936	3.682152
215.570553	4591.195148	7.128960	-0.042998	3.685218
215.746927	4599.253797	7.133965	-0.043036	3.688305
215.875392	4607.287299	7.138970	-0.043066	3.691378
216.233725	4615.338623	7.143974	-0.043137	3.694462
216.213179	4623.337353	7.148979	-0.043139	3.697513
216.433917	4631.344124	7.153984	-0.043185	3.700570
216.848076	4639.366340	7.158989	-0.043268	3.703636
216.973848	4647.364887	7.163994	-0.043296	3.706683
217.362717	4655.426961	7.168998	-0.043374	3.709758
217.392737	4663.506747	7.174003	-0.043385	3.712829
217.519255	4671.546715	7.179008	-0.043413	3.715884
217.872237	4679.540126	7.184013	-0.043484	3.718925
217.891951	4687.488222	7.189018	-0.043493	3.721937
218.226258	4695.502706	7.194022	-0.043561	3.724980
218.540557	4703.530125	7.199027	-0.043624	3.728025
218.489869	4711.577481	7.204032	-0.043620	3.731066
218.797383	4719.597169	7.209037	-0.043683	3.734103
218.992578	4727.619022	7.214042	-0.043724	3.737136
219.335782	4735.658890	7.219046	-0.043793	3.740176
219.469274	4743.652283	7.224051	-0.043824	3.743191
219.943961	4751.656601	7.229056	-0.043917	3.746216
220.310359	4759.686798	7.234061	-0.043991	3.749246
220.297185	4767.764655	7.239066	-0.043993	3.752282
220.825000	4775.777348	7.244070	-0.044097	3.755303
220.995636	4783.757168	7.249075	-0.044134	3.758302
221.322192	4791.807990	7.254080	-0.044200	3.761329
221.533236	4799.830011	7.259085	-0.044244	3.764339
221.738554	4807.841383	7.264090	-0.044288	3.767343
222.272506	4815.866797	7.269094	-0.044393	3.770357
222.505214	4823.867015	7.274099	-0.044441	3.773353
222.799142	4831.951116	7.279104	-0.044501	3.776379
222.908532	4839.959223	7.284109	-0.044527	3.779370
223.235259	4847.938892	7.289114	-0.044593	3.782352
223.302905	4855.964836	7.294118	-0.044611	3.785344
223.414462	4863.997901	7.299123	-0.044637	3.788337
223.572856	4872.054738	7.304128	-0.044671	3.791338
223.792142	4880.124507	7.309133	-0.044717	3.794342
223.882650	4888.108315	7.314138	-0.044739	3.797309
224.289899	4896.083959	7.319142	-0.044820	3.800278
224.385516	4904.082640	7.324147	-0.044843	3.803246
224.506563	4912.098773	7.329152	-0.044871	3.806219
224.925863	4920.119019	7.334157	-0.044955	3.809197
225.071610	4928.151506	7.339162	-0.044987	3.812172
225.414559	4936.227071	7.344166	-0.045056	3.815164
225.661817	4944.186975	7.349171	-0.045107	3.818110
225.714669	4952.240490	7.354176	-0.045122	3.821083
226.045385	4960.218311	7.359181	-0.045189	3.824032
226.135452	4968.275528	7.364186	-0.045211	3.827003
226.380431	4976.287815	7.369190	-0.045262	3.829958
226.497424	4984.354417	7.374195	-0.045289	3.832929
226.636204	4992.356438	7.379200	-0.045320	3.835873
227.078988	5000.336482	7.384205	-0.045408	3.838814
227.338414	5008.360373	7.389210	-0.045461	3.841765
227.429394	5016.359111	7.394214	-0.045483	3.844700
227.636024	5024.406983	7.399219	-0.045527	3.847654
228.129722	5032.391444	7.404224	-0.045624	3.850588
228.158694	5040.486487	7.409229	-0.045635	3.853551
228.435929	5048.489511	7.414234	-0.045692	3.856483
228.886131	5056.490946	7.419238	-0.045781	3.859415
228.704784	5064.585474	7.424243	-0.045752	3.862367
228.834444	5072.528729	7.429248	-0.045782	3.865267
229.282880	5080.608026	7.434253	-0.045870	3.868221
229.407567	5088.616941	7.439258	-0.045899	3.871141
229.548206	5096.896253	7.444262	-0.045930	3.874157
229.576525	5104.841194	7.449267	-0.045941	3.877047
229.913798	5112.734255	7.454272	-0.046009	3.879922
230.213984	5120.766891	7.459277	-0.046070	3.882845
230.216893	5128.695887	7.464282	-0.046076	3.885722
230.629510	5136.746839	7.469286	-0.046158	3.888649
230.857157	5144.770723	7.474291	-0.046205	3.891561
230.841376	5152.792840	7.479296	-0.046208	3.894465
231.009362	5160.833747	7.484301	-0.046244	3.897377
231.231382	5168.803623	7.489306	-0.046291	3.900262
231.448323	5176.847205	7.494310	-0.046336	3.903172
231.569496	5184.849946	7.499315	-0.046364	3.906063
231.993671	5192.847337	7.504320	-0.046448	3.908956
232.253813	5200.906082	7.509325	-0.046502	3.911865
232.290779	5208.947711	7.514330	-0.046514	3.914762
232.458617	5216.940899	7.519334	-0.046551	3.917642
232.761199	5224.940133	7.524339	-0.046612	3.920524
232.766989	5232.914383	7.529344	-0.046618	3.923390
233.071569	5240.994180	7.534349	-0.046680	3.926296
233.266603	5248.979429	7.539354	-0.046722	3.929165
233.431076	5257.043561	7.544358	-0.046758	3.932060
233.439304	5265.077062	7.549363	-0.046764	3.934938
233.632944	5273.094146	7.554368	-0.046806	3.937812
234.120612	5281.094747	7.559373	-0.046902	3.940683
234.107266	5289.057116	7.564378	-0.046904	3.943529
234.343387	5297.130120	7.569382	-0.046954	3.946417
234.598705	5305.137340	7.574387	-0.047006	3.949280
234.607751	5313.169504	7.579392	-0.047013	3.952146
234.954615	5321.219132	7.584397	-0.047083	3.955021
235.203133	5329.200619	7.589402	-0.047135	3.957868
235.489582	5337.198423	7.594406	-0.047193	3.960720
235.400010	5345.202607	7.599411	-0.047182	3.963565
235.496174	5353.224722	7.604416	-0.047205	3.966418
236.060559	5361.245315	7.609421	-0.047315	3.969276
235.947657	5369.305812	7.614426	-0.047299	3.972135
236.365120	5377.334701	7.619430	-0.047382	3.974990
236.657359	5385.347235	7.624435	-0.047442	3.977834
236.725691	5393.349664	7.629440	-0.047460	3.980669
236.743852	5401.382237	7.634445	-0.047469	3.983512
237.011289	5409.385140	7.639450	-0.047524	3.986347
237.661361	5417.423006	7.644454	-0.047650	3.989198
237.721432	5425.472848	7.649459	-0.047666	3.992041
237.732454	5433.516551	7.654464	-0.047674	3.994880
238.015000	5441.558903	7.659469	-0.047731	3.997720
238.097725	5449.543507	7.664474	-0.047752	4.000535
238.187776	5457.568035	7.669478	-0.047774	4.003362
238.322479	5465.559878	7.674483	-0.047804	4.006176
238.573078	5473.553089	7.679488	-0.047856	4.008991
238.513674	5481.628104	7.684493	-0.047850	4.011827
238.747234	5489.646859	7.689498	-0.047899	4.014646
239.031112	5497.653105	7.694502	-0.047957	4.017460
239.165189	5505.666352	7.699507	-0.047987	4.020271
239.344564	5513.679719	7.704512	-0.048026	4.023082
239.691349	5521.699481	7.709517	-0.048096	4.025895
239.806280	5529.719028	7.714522	-0.048122	4.028703
239.909617	5537.772419	7.719526	-0.048147	4.031520
240.192453	5545.881855	7.724531	-0.048205	4.034357
240.449680	5553.905197	7.729536	-0.048258	4.037163
240.654109	5561.795955	7.734541	-0.048301	4.039919
240.727595	5569.807941	7.739546	-0.048320	4.042713
241.320804	5577.804395	7.744550	-0.048436	4.045508
241.198090	5585.831431	7.749555	-0.048418	4.048301
241.386242	5593.874262	7.754560	-0.048458	4.051102
241.750724	5601.927956	7.759565	-0.048532	4.053907
241.708061	5609.920719	7.764570	-0.048529	4.056684
242.032362	5617.904662	7.769574	-0.048594	4.059461
242.256656	5625.920836	7.774579	-0.048641	4.062245
242.291349	5633.923360	7.779584	-0.048653	4.065020
242.491568	5642.006646	7.784589	-0.048696	4.067824
242.615834	5649.978719	7.789594	-0.048724	4.070586
243.152225	5658.026265	7.794598	-0.048829	4.073378
243.309252	5666.046946	7.799603	-0.048863	4.076153
243.222746	5674.058506	7.804608	-0.048853	4.078920
243.657697	5682.098129	7.809613	-0.048939	4.081702
243.777232	5690.037357	7.814618	-0.048966	4.084443
243.832131	5698.104981	7.819622	-0.048982	4.087226
243.959501	5706.081033	7.824627	-0.049011	4.089976
244.305808	5714.132870	7.829632	-0.049080	4.092754
244.546744	5722.207127	7.834637	-0.049130	4.095535
244.661057	5730.163822	7.839642	-0.049157	4.098273
245.044565	5738.185517	7.844646	-0.049234	4.101035
245.146882	5746.186257	7.849651	-0.049258	4.103784
245.101730	5754.246257	7.854656	-0.049255	4.106549
245.406878	5762.261077	7.859661	-0.049317	4.109302
245.698583	5770.276444	7.864666	-0.049376	4.112053
245.997224	5778.346288	7.869670	-0.049437	4.114820
246.086035	5786.395757	7.874675	-0.049459	4.117576
246.435036	5794.314093	7.879680	-0.049529	4.120289
246.666558	5802.360915	7.884685	-0.049577	4.123042
246.626348	5810.356444	7.889690	-0.049575	4.125773
247.125329	5818.403455	7.894694	-0.049673	4.128526
247.195479	5826.410279	7.899699	-0.049692	4.131258
247.286173	5834.438188	7.904704	-0.049714	4.133996
247.705917	5842.533905	7.909709	-0.049797	4.136758
247.585289	5850.473792	7.914714	-0.049780	4.139460
247.690730	5858.554916	7.919718	-0.049805	4.142210
247.825841	5866.520077	7.924723	-0.049835	4.144920
248.142809	5874.563175	7.929728	-0.049899	4.147656
248.335721	5882.570986	7.934733	-0.049940	4.150378
248.350346	5890.595858	7.939738	-0.049948	4.153101
248.688347	5898.655362	7.944742	-0.050017	4.155837
248.836737	5906.651264	7.949747	-0.050049	4.158549
248.945107	5914.621541	7.954752	-0.050075	4.161249
249.307523	5922.629023	7.959757	-0.050148	4.163963
249.369792	5930.694502	7.964762	-0.050164	4.166691
249.499900	5938.681704	7.969766	-0.050194	4.169392
249.864443	5946.732897	7.974771	-0.050267	4.172115
250.045116	5954.741943	7.979776	-0.050306	4.174820
250.156441	5962.751146	7.984781	-0.050332	4.177523
250.398761	5970.744616	7.989786	-0.050382	4.180220
250.432383	5978.790952	7.994790	-0.050394	4.182931
250.845183	5986.752312	7.999795	-0.050476	4.185616
250.836766	5994.765949	8.004800	-0.050479	4.188312
251.235364	6002.847891	8.009805	-0.050559	4.191033
251.265900	6010.952549	8.014810	-0.050570	4.193756
251.625645	6018.967441	8.019814	-0.050642	4.196451
251.553225	6026.883952	8.024819	-0.050634	4.199107
251.829849	6034.941697	8.029824	-0.050690	4.201812
252.037934	6042.903439	8.034829	-0.050734	4.204482
252.107109	6050.911920	8.039834	-0.050752	4.207165
252.267292	6058.936756	8.044838	-0.050787	4.209852
252.630427	6066.955942	8.049843	-0.050860	4.212538
252.738083	6074.973185	8.054848	-0.050886	4.215219
253.160304	6083.034741	8.059853	-0.050969	4.217916
253.323089	6090.989640	8.064858	-0.051005	4.220573
253.344463	6099.017478	8.069862	-0.051014	4.223251
253.501724	6107.008954	8.074867	-0.051049	4.225917
253.898919	6115.042573	8.079872	-0.051128	4.228598
253.906843	6123.103103	8.084877	-0.051135	4.231282
253.918880	6131.126409	8.089882	-0.051142	4.233952
254.195263	6139.155656	8.094886	-0.051199	4.236624
254.477462	6147.117571	8.099891	-0.051256	4.239273
254.363943	6155.152210	8.104896	-0.051241	4.241941
254.593050	6163.133305	8.109901	-0.051288	4.244592
254.780066	6171.171507	8.114906	-0.051328	4.247260
254.915570	6179.173882	8.119910	-0.051359	4.249914
255.067292	6187.265716	8.124915	-0.051392	4.252596
255.378526	6195.255550	8.129920	-0.051456	4.255244
255.511559	6203.312908	8.134925	-0.051486	4.257911
255.545635	6211.296823	8.139930	-0.051497	4.260552
255.799792	6219.328966	8.144934	-0.051550	4.263208
256.215068	6227.316558	8.149939	-0.051632	4.265850
256.249394	6235.296612	8.154944	-0.051644	4.268484
256.555773	6243.378648	8.159949	-0.051706	4.271152
256.844652	6251.445482	8.164954	-0.051765	4.273813
256.993184	6259.483167	8.169958	-0.051798	4.276463
257.128406	6267.431382	8.174963	-0.051828	4.279080
257.285664	6275.483632	8.179968	-0.051863	4.281731
257.570386	6283.428506	8.184973	-0.051921	4.284346
257.687630	6291.475680	8.189978	-0.051948	4.286991
257.874418	6299.436762	8.194982	-0.051988	4.289607
258.138616	6307.541713	8.199987	-0.052043	4.292269
258.327604	6315.540340	8.204992	-0.052083	4.294894
258.360462	6323.602985	8.209997	-0.052094	4.297537
258.566092	6331.562551	8.215002	-0.052138	4.300146
258.767626	6339.592005	8.220006	-0.052181	4.302776
259.033033	6347.605860	8.225011	-0.052235	4.305400
258.914751	6355.624164	8.230016	-0.052218	4.308021
259.393104	6363.643952	8.235021	-0.052313	4.310646
259.504627	6371.724142	8.240026	-0.052339	4.313285
259.639881	6379.693012	8.245030	-0.052369	4.315887
259.779947	6387.694410	8.250035	-0.052400	4.318498
260.003967	6395.721820	8.255040	-0.052447	4.321117
260.128878	6403.689302	8.260045	-0.052476	4.323713
260.225691	6411.750496	8.265050	-0.052499	4.326338
260.709874	6419.706421	8.270054	-0.052594	4.328931
260.651916	6427.787595	8.275059	-0.052589	4.331558
260.661273	6435.828010	8.280064	-0.052596	4.334171
260.988004	6443.821337	8.285069	-0.052662	4.336770
260.966357	6451.782693	8.290074	-0.052663	4.339354
261.118886	6459.876076	8.295078	-0.052697	4.341980
261.486733	6467.851486	8.300083	-0.052771	4.344568
261.687661	6475.829449	8.305088	-0.052813	4.347155
262.128783	6483.895132	8.310093	-0.052901	4.349769
262.428041	6491.931074	8.315098	-0.052961	4.352372
262.581925	6500.011545	8.320102	-0.052995	4.354986
262.697967	6508.020393	8.325107	-0.053022	4.357576
263.117850	6515.956580	8.330112	-0.053106	4.360142
263.296636	6523.980637	8.335117	-0.053144	4.362733
263.493878	6531.941437	8.340122	-0.053186	4.365303
263.361861	6539.991704	8.345126	-0.053167	4.367898
263.741314	6548.011920	8.350131	-0.053243	4.370485
263.920782	6556.005853	8.355136	-0.053281	4.373061
264.181863	6564.088460	8.360141	-0.053335	4.375664
264.403180	6572.071868	8.365146	-0.053381	4.378233
264.512023	6580.101910	8.370150	-0.053407	4.380815
264.688058	6588.081116	8.375155	-0.053445	4.383380
264.658712	6596.071605	8.380160	-0.053445	4.385946
265.197428	6604.158088	8.385165	-0.053550	4.388544
265.337704	6612.166861	8.390170	-0.053582	4.391113
265.427202	6620.199763	8.395174	-0.053603	4.393689
265.444181	6628.263012	8.400179	-0.053612	4.396272
265.623450	6636.186885	8.405184	-0.053650	4.398810
265.798436	6644.263834	8.410189	-0.053688	4.401395
265.954058	6652.221899	8.415194	-0.053722	4.403941
266.362172	6660.287098	8.420198	-0.053804	4.406520
266.601575	6668.290448	8.425203	-0.053853	4.409078
266.551284	6676.329494	8.430208	-0.053849	4.411644
266.719574	6684.403112	8.435213	-0.053886	4.414221
266.859361	6692.386952	8.440218	-0.053917	4.416767
266.959612	6700.364297	8.445222	-0.053941	4.419309
267.384771	6708.402250	8.450227	-0.054025	4.421871
267.472995	6716.335189	8.455232	-0.054047	4.424397
267.601433	6724.439995	8.460237	-0.054076	4.426976
267.709946	6732.436906	8.465242	-0.054102	4.429518
268.128672	6740.479306	8.470246	-0.054185	4.432076
268.251456	6748.508016	8.475251	-0.054213	4.434626
268.230423	6756.473509	8.480256	-0.054214	4.437154
268.503532	6764.487817	8.485261	-0.054270	4.439697
268.773642	6772.512786	8.490266	-0.054326	4.442242
268.963860	6780.437063	8.495270	-0.054366	4.444753
269.144777	6788.585965	8.500275	-0.054405	4.447334
269.379905	6796.515962	8.505280	-0.054454	4.449844
269.445328	6804.638297	8.510285	-0.054472	4.452414
269.328515	6812.603598	8.515290	-0.054455	4.454931
269.675056	6820.655723	8.520294	-0.054525	4.457476
270.075925	6828.605122	8.525299	-0.054605	4.459987
269.877158	6836.601839	8.530304	-0.054573	4.462510
270.230929	6844.639208	8.535309	-0.054644	4.465046
270.247847	6852.690073	8.540314	-0.054653	4.467583
270.345802	6860.701997	8.545318	-0.054676	4.470108
270.545567	6868.735234	8.550323	-0.054718	4.472637
270.880716	6876.748820	8.555328	-0.054786	4.475160
270.974986	6884.765643	8.560333	-0.054809	4.477681
271.022575	6892.758698	8.565338	-0.054823	4.480193
271.381885	6900.777946	8.570343	-0.054895	4.482714
271.581401	6908.777589	8.575347	-0.054937	4.485226
271.662963	6916.779972	8.580352	-0.054958	4.487737
271.958078	6924.816695	8.585357	-0.055018	4.490258
272.017576	6932.850312	8.590362	-0.055034	4.492775
272.230333	6940.862128	8.595367	-0.055079	4.495286
272.503652	6948.890937	8.600371	-0.055135	4.497800
272.885682	6956.878478	8.605376	-0.055212	4.500300
272.897834	6964.913758	8.610381	-0.055219	4.502812
273.056169	6972.875363	8.615386	-0.055254	4.505301
273.250674	6980.922127	8.620391	-0.055295	4.507815
273.548031	6988.954633	8.625395	-0.055356	4.510323
273.449570	6996.990838	8.630400	-0.055343	4.512830
273.762162	7005.064389	8.635405	-0.055406	4.515348
273.961024	7013.056247	8.640410	-0.055448	4.517839
273.998456	7020.979578	8.645415	-0.055461	4.520307
274.080100	7029.018302	8.650419	-0.055481	4.522810
274.352331	7036.998980	8.655424	-0.055537	4.525293
274.563232	7045.061897	8.660429	-0.055581	4.527801
274.568603	7053.058358	8.665434	-0.055588	4.530286
274.849080	7061.048440	8.670439	-0.055645	4.532768
275.093111	7069.136798	8.675443	-0.055696	4.535280
275.109392	7077.100237	8.680448	-0.055704	4.537750
275.280234	7085.118509	8.685453	-0.055741	4.540237
275.389581	7093.131515	8.690458	-0.055767	4.542721
275.548180	7101.085178	8.695463	-0.055801	4.545185
275.583159	7109.178023	8.700467	-0.055813	4.547690
275.818057	7117.151232	8.705472	-0.055862	4.550157
276.026452	7125.256237	8.710477	-0.055906	4.552664
276.171824	7133.238770	8.715482	-0.055938	4.555131
276.291562	7141.299609	8.720487	-0.055966	4.557621
276.624768	7149.261862	8.725491	-0.056033	4.560080
276.606875	7157.273456	8.730496	-0.056035	4.562552
276.815875	7165.258164	8.735501	-0.056079	4.565015
277.072786	7173.334237	8.740506	-0.056132	4.567504
277.136491	7181.311059	8.745511	-0.056149	4.569961
277.272493	7189.388336	8.750515	-0.056180	4.572448
277.361534	7197.342340	8.755520	-0.056202	4.574896
277.704487	7205.439050	8.760525	-0.056271	4.577386
277.636307	7213.371710	8.765530	-0.056263	4.579825
277.920134	7221.444963	8.770535	-0.056321	4.582305
278.120330	7229.415086	8.775539	-0.056364	4.584752
278.338779	7237.454643	8.780544	-0.056410	4.587220
278.440868	7245.475415	8.785549	-0.056434	4.589680
278.734233	7253.548109	8.790554	-0.056494	4.592155
278.880595	7261.562294	8.795559	-0.056526	4.594610
278.856550	7269.602455	8.800563	-0.056527	4.597072
278.991697	7277.489626	8.805568	-0.056557	4.599486
279.242008	7285.595294	8.810573	-0.056609	4.601966
279.348257	7293.482852	8.815578	-0.056634	4.604377
279.520963	7301.522754	8.820583	-0.056672	4.606834
279.851086	7309.564939	8.825587	-0.056738	4.609290
279.884811	7317.581896	8.830592	-0.056750	4.611737
279.986150	7325.674797	8.835597	-0.056774	4.614206
280.064681	7333.674774	8.840602	-0.056794	4.616645
280.276537	7341.614531	8.845607	-0.056838	4.619065
280.324290	7349.725544	8.850611	-0.056853	4.621535
280.643684	7357.666781	8.855616	-0.056917	4.623952
280.936142	7365.706702	8.860621	-0.056977	4.626398
281.038878	7373.707620	8.865626	-0.057001	4.628831
281.156656	7381.751862	8.870631	-0.057028	4.631276
281.499586	7389.802848	8.875635	-0.057098	4.633722
281.643719	7397.772479	8.880640	-0.057130	4.636141
281.737656	7405.764756	8.885645	-0.057152	4.638566
281.969920	7413.742012	8.890650	-0.057201	4.640986
282.127985	7421.795459	8.895655	-0.057235	4.643427
282.219467	7429.800467	8.900659	-0.057258	4.645852
282.330932	7437.822133	8.905664	-0.057284	4.648281
282.873043	7445.866909	8.910669	-0.057390	4.650715
282.918644	7453.904174	8.915674	-0.057404	4.653146
282.962554	7461.892982	8.920679	-0.057417	4.655561
283.299030	7469.901501	8.925683	-0.057485	4.657981
283.469566	7477.895071	8.930688	-0.057522	4.660395
283.502660	7485.957481	8.935693	-0.057533	4.662828
283.642767	7493.909682	8.940698	-0.057564	4.665227
283.898504	7501.984612	8.945703	-0.057617	4.667662
283.917956	7509.985058	8.950707	-0.057626	4.670073
284.035715	7518.064772	8.955712	-0.057653	4.672507
284.455439	7526.121224	8.960717	-0.057737	4.674932
284.699244	7534.102239	8.965722	-0.057787	4.677333
284.709154	7542.014545	8.970727	-0.057794	4.679712
285.044435	7550.087507	8.975731	-0.057862	4.682138
285.116212	7557.981366	8.980736	-0.057881	4.684510
285.341656	7566.080892	8.985741	-0.057928	4.686942
285.624394	7574.068538	8.990746	-0.057986	4.689338
285.911699	7582.113511	8.995751	-0.058044	4.691751
285.875769	7590.158534	9.000755	-0.058043	4.694163
286.043970	7598.138207	9.005760	-0.058079	4.696554
286.343283	7606.120846	9.010765	-0.058140	4.698944
286.592548	7614.165734	9.015770	-0.058192	4.701352
286.616426	7622.144305	9.020775	-0.058202	4.703739
286.938700	7630.176192	9.025779	-0.058267	4.706140
287.009161	7638.191556	9.030784	-0.058285	4.708536
287.232679	7646.249884	9.035789	-0.058332	4.710942
287.495659	7654.276143	9.040794	-0.058386	4.713338
287.624290	7662.288733	9.045799	-0.058415	4.715729
287.732788	7670.334590	9.050803	-0.058441	4.718129
287.893491	7678.270870	9.055808	-0.058476	4.720494
288.308220	7686.362287	9.060813	-0.058559	4.722904
288.412447	7694.333539	9.065818	-0.058583	4.725278
288.306573	7702.332071	9.070823	-0.058569	4.727659
288.618833	7710.380561	9.075827	-0.058632	4.730052
288.841631	7718.397733	9.080832	-0.058679	4.732436
288.834473	7726.433576	9.085837	-0.058683	4.734824
288.897065	7734.488903	9.090842	-0.058700	4.737217
289.215090	7742.410023	9.095847	-0.058764	4.739568
289.494380	7750.476861	9.100851	-0.058821	4.741961
289.572795	7758.420457	9.105856	-0.058841	4.744316
289.903140	7766.481381	9.110861	-0.058908	4.746705
290.064867	7774.506694	9.115866	-0.058943	4.749083
290.125431	7782.512816	9.120871	-0.058960	4.751453
290.230346	7790.632139	9.125875	-0.058984	4.753856
290.499374	7798.569649	9.130880	-0.059040	4.756204
290.788273	7806.540995	9.135885	-0.059099	4.758560
290.768243	7814.564463	9.140890	-0.059100	4.760931
290.828134	7822.523141	9.145895	-0.059116	4.763282
291.092392	7830.611006	9.150899	-0.059171	4.765669
291.003056	7838.585349	9.155904	-0.059159	4.768023
291.241340	7846.609094	9.160909	-0.059209	4.770389
291.407515	7854.650811	9.165914	-0.059245	4.772759
291.650073	7862.628724	9.170919	-0.059296	4.775109
292.070823	7870.684093	9.175923	-0.059379	4.777480
292.180037	7878.622708	9.180928	-0.059405	4.779816
292.304418	7886.726789	9.185933	-0.059433	4.782200
292.389869	7894.643289	9.190938	-0.059454	4.784528
292.762394	7902.764298	9.195943	-0.059529	4.786914
293.193361	7910.737289	9.200947	-0.059614	4.789254
293.000800	7918.772262	9.205952	-0.059584	4.791615
293.216042	7926.822474	9.210957	-0.059629	4.793976
293.416371	7934.859491	9.215962	-0.059672	4.796333
293.607866	7942.763021	9.220967	-0.059712	4.798650
294.177716	7950.869128	9.225971	-0.059824	4.801023
294.333062	7958.808846	9.230976	-0.059858	4.803348
294.523615	7966.861828	9.235981	-0.059899	4.805704
294.745437	7974.843575	9.240986	-0.059945	4.808039
295.122838	7982.858496	9.245991	-0.060021	4.810382
295.390261	7990.453739	9.250995	-0.060075	4.812601
295.346559	7995.143037	9.256000	-0.060070	4.813971
295.645992	7997.746757	9.261005	-0.060128	4.814730
295.862330	7999.084087	9.266010	-0.060169	4.815120
295.957639	7999.520656	9.271015	-0.060187	4.815247
296.047145	8000.178390	9.276019	-0.060204	4.815439
296.156043	8000.422822	9.281024	-0.060224	4.815510
296.228156	8000.301098	9.286029	-0.060238	4.815474
296.190689	8000.402018	9.291034	-0.060231	4.815503
296.267600	8000.384053	9.296039	-0.060245	4.815498
296.514955	8000.396703	9.301043	-0.060291	4.815500
296.531367	8000.238784	9.306048	-0.060294	4.815454
296.646784	8000.282381	9.311053	-0.060316	4.815466
296.820272	8000.388936	9.316058	-0.060348	4.815497
296.929199	8000.310576	9.321063	-0.060368	4.815473
296.910133	8000.258954	9.326067	-0.060365	4.815458
296.859282	8000.328657	9.331072	-0.060355	4.815479
296.941403	8000.184652	9.336077	-0.060370	4.815436
296.601553	8000.196123	9.341082	-0.060307	4.815441
296.852793	8000.371303	9.346087	-0.060354	4.815491
296.939977	8000.277619	9.351091	-0.060370	4.815464
297.072617	8000.467939	9.356096	-0.060395	4.815518
297.113690	8000.165060	9.361101	-0.060403	4.815430
297.128295	8000.216607	9.366106	-0.060405	4.815445
297.129482	8000.321376	9.371111	-0.060406	4.815475
297.231164	8000.037674	9.376115	-0.060424	4.815392
297.169749	8000.251498	9.381120	-0.060413	4.815455
297.403699	8000.179485	9.386125	-0.060457	4.815433
297.414359	8000.257689	9.391130	-0.060459	4.815455
297.304629	8000.158603	9.396135	-0.060438	4.815427
297.395788	8000.171871	9.401139	-0.060455	4.815430
297.251852	8000.219723	9.406144	-0.060428	4.815445
297.377591	8000.300903	9.411149	-0.060452	4.815468
297.436576	8000.322190	9.416154	-0.060463	4.815474
297.405059	8000.369767	9.421159	-0.060457	4.815488
297.638463	8000.326605	9.426163	-0.060500	4.815474
297.620972	8000.176672	9.431168	-0.060497	4.815431
297.638656	8000.276370	9.436173	-0.060500	4.815460
297.835926	8000.174890	9.441178	-0.060537	4.815429
297.705277	8000.356572	9.446183	-0.060513	4.815483
297.784628	8000.038292	9.451187	-0.060527	4.815390
297.574520	8000.279582	9.456192	-0.060488	4.815461
297.636256	8000.300914	9.461197	-0.060500	4.815467
297.665429	8000.209474	9.466202	-0.060505	4.815440
297.775348	8000.296806	9.471207	-0.060526	4.815465
297.705071	8000.145998	9.476211	-0.060513	4.815421
297.646234	8000.416519	9.481216	-0.060502	4.815501
297.783667	8000.135543	9.486221	-0.060527	4.815418
297.820292	8000.243038	9.491226	-0.060534	4.815449
297.747503	8000.352995	9.496231	-0.060521	4.815482
298.104062	8000.093822	9.501235	-0.060587	4.815404
298.031812	8000.281817	9.506240	-0.060573	4.815459
297.984038	8000.161310	9.511245	-0.060565	4.815424
298.050156	8000.270363	9.516250	-0.060577	4.815456
298.121873	8000.239485	9.521255	-0.060590	4.815447
298.042120	8000.034006	9.526259	-0.060575	4.815387
298.000730	8000.102797	9.531264	-0.060568	4.815407
298.072862	8000.170263	9.536269	-0.060581	4.815427
298.231444	8000.134412	9.541274	-0.060611	4.815415
298.093160	8000.154566	9.546279	-0.060585	4.815422
298.315628	8000.106948	9.551283	-0.060626	4.815407
298.217691	8000.253900	9.556288	-0.060608	4.815450
298.250659	8000.223448	9.561293	-0.060614	4.815441
298.309999	8000.060892	9.566298	-0.060625	4.815394
298.433886	8000.222210	9.571303	-0.060648	4.815440
298.574115	8000.190331	9.576307	-0.060674	4.815430
298.533559	8000.297617	9.581312	-0.060667	4.815462
298.510170	8000.081312	9.586317	-0.060662	4.815399
298.422483	8000.054204	9.591322	-0.060646	4.815391
298.328109	8000.074018	9.596327	-0.060629	4.815397
298.404077	7999.996179	9.601331	-0.060643	4.815374
298.495782	8000.145206	9.606336	-0.060660	4.815417
298.338449	8000.143666	9.611341	-0.060630	4.815418
298.381615	8000.193551	9.616346	-0.060639	4.815432
298.520018	8000.166985	9.621351	-0.060664	4.815424
298.520985	8000.222584	9.626355	-0.060665	4.815440
298.345561	8000.299843	9.631360	-0.060632	4.815463
298.383873	8000.112352	9.636365	-0.060639	4.815408
298.608231	8000.205859	9.641370	-0.060681	4.815434
298.619995	8000.380286	9.646375	-0.060683	4.815485
298.781395	8000.213006	9.651379	-0.060713	4.815436
298.567286	8000.287485	9.656384	-0.060673	4.815459
298.745178	8000.003970	9.661389	-0.060706	4.815375
298.959387	8000.160374	9.666394	-0.060746	4.815419
298.845417	8000.269650	9.671399	-0.060725	4.815452
299.088098	8000.068444	9.676403	-0.060770	4.815392
298.755568	8000.323743	9.681408	-0.060708	4.815468
298.893230	8000.149656	9.686413	-0.060734	4.815417
298.992420	8000.143818	9.691418	-0.060752	4.815414
298.640238	8000.130496	9.696423	-0.060687	4.815412
298.740457	8000.122538	9.701427	-0.060705	4.815409
298.916614	8000.290070	9.706432	-0.060738	4.815458
299.002997	8000.335329	9.711437	-0.060754	4.815470
298.798495	8000.217563	9.716442	-0.060716	4.815437
298.864187	8000.463434	9.721447	-0.060729	4.815508
298.987934	8000.207878	9.726451	-0.060751	4.815433
298.795572	8000.236755	9.731456	-0.060716	4.815443
298.640982	8000.297256	9.736461	-0.060687	4.815461
298.710210	8000.288784	9.741466	-0.060700	4.815458
298.673573	8000.294590	9.746471	-0.060693	4.815460
298.921205	8000.011161	9.751475	-0.060739	4.815376
299.072347	8000.192174	9.756480	-0.060767	4.815428
299.030183	8000.018312	9.761485	-0.060759	4.815378
298.915663	8000.179955	9.766490	-0.060738	4.815425
298.920724	8000.323273	9.771495	-0.060739	4.815467
299.070421	8000.093802	9.776499	-0.060767	4.815399
298.913930	8000.188477	9.781504	-0.060738	4.815428
298.744880	8000.278669	9.786509	-0.060706	4.815455
298.847258	8000.147822	9.791514	-0.060725	4.815416
298.881936	8000.249943	9.796519	-0.060732	4.815446
298.842358	8000.085744	9.801523	-0.060724	4.815398
298.813569	8000.244533	9.806528	-0.060719	4.815445
298.928559	8000.222924	9.811533	-0.060740	4.815438
299.050184	8000.214252	9.816538	-0.060763	4.815435
299.016620	8000.203006	9.821543	-0.060757	4.815432
299.128972	8000.201662	9.826547	-0.060778	4.815431
298.875017	8000.110869	9.831552	-0.060730	4.815405
299.073085	8000.245630	9.836557	-0.060767	4.815444
298.995267	8000.175928	9.841562	-0.060753	4.815424
298.880201	8000.224259	9.846567	-0.060731	4.815439
298.904307	8000.255657	9.851571	-0.060736	4.815448
298.971413	8000.209738	9.856576	-0.060748	4.815434
298.994460	8000.079713	9.861581	-0.060752	4.815396
298.749461	8000.117338	9.866586	-0.060707	4.815408
298.912265	8000.372300	9.871591	-0.060737	4.815482
299.184959	8000.173729	9.876595	-0.060788	4.815422
298.950181	8000.083254	9.881600	-0.060744	4.815397
298.908159	8000.190516	9.886605	-0.060736	4.815429
299.054289	8000.134149	9.891610	-0.060764	4.815411
299.015418	8000.082197	9.896615	-0.060756	4.815396
299.128335	8000.046658	9.901619	-0.060777	4.815385
299.118835	8000.166218	9.906624	-0.060776	4.815420
299.150092	7999.950817	9.911629	-0.060781	4.815357
299.265288	8000.132303	9.916634	-0.060803	4.815410
299.040641	8000.216228	9.921639	-0.060761	4.815435
299.228005	8000.018380	9.926643	-0.060796	4.815377
298.968426	8000.247098	9.931648	-0.060748	4.815445
298.953009	8000.170949	9.936653	-0.060745	4.815423
298.996601	8000.143880	9.941658	-0.060753	4.815414
299.122894	8000.231488	9.946663	-0.060776	4.815439
299.086350	7999.963655	9.951667	-0.060769	4.815361
299.061723	8000.273230	9.956672	-0.060765	4.815452
299.006696	8000.114118	9.961677	-0.060755	4.815406
299.053039	8000.094577	9.966682	-0.060763	4.815400
299.012016	8000.133446	9.971687	-0.060756	4.815411
299.086656	8000.180647	9.976691	-0.060770	4.815425
299.128366	8000.107584	9.981696	-0.060777	4.815403
299.011994	8000.154823	9.986701	-0.060756	4.815418
299.198569	8000.137608	9.991706	-0.060790	4.815412
299.202556	8000.221050	9.996711	-0.060791	4.815436
299.007873	8000.074587	10.001715	-0.060755	4.815394
299.051485	8000.124479	10.006720	-0.060763	4.815409
299.246087	8000.156567	10.011725	-0.060799	4.815417
299.189425	8000.060494	10.016730	-0.060789	4.815389
299.147275	8000.181651	10.021735	-0.060781	4.815425
299.387213	8000.023155	10.026739	-0.060826	4.815377
299.253450	8000.233651	10.031744	-0.060801	4.815439
299.089732	7999.982949	10.036749	-0.060770	4.815367
299.157433	8000.133718	10.041754	-0.060783	4.815411
299.205854	8000.104591	10.046759	-0.060792	4.815402
299.095499	7999.959528	10.051763	-0.060771	4.815360
299.208693	8000.129223	10.056768	-0.060792	4.815409
299.237402	8000.170318	10.061773	-0.060798	4.815421
299.162454	8000.141283	10.066778	-0.060784	4.815413
299.058076	8000.182308	10.071783	-0.060764	4.815425
299.242185	8000.076332	10.076787	-0.060799	4.815394
299.293696	8000.129563	10.081792	-0.060808	4.815409
299.286658	8000.181823	10.086797	-0.060807	4.815424
299.471751	8000.168859	10.091802	-0.060841	4.815419
299.530901	8000.277802	10.096807	-0.060852	4.815451
299.411710	8000.059902	10.101811	-0.060830	4.815388
299.333189	8000.116321	10.106816	-0.060816	4.815405
299.359315	8000.056895	10.111821	-0.060820	4.815387
299.446010	8000.230429	10.116826	-0.060837	4.815438
299.191651	8000.053046	10.121831	-0.060789	4.815387
299.228043	8000.069683	10.126835	-0.060796	4.815392
299.423514	8000.100716	10.131840	-0.060832	4.815400
299.288175	8000.117712	10.136845	-0.060807	4.815405
299.288015	8000.001198	10.141850	-0.060807	4.815371
299.313805	8000.157686	10.146855	-0.060812	4.815417
299.302505	8000.177808	10.151859	-0.060810	4.815423
299.393031	8000.326821	10.156864	-0.060827	4.815466
299.405988	8000.265038	10.161869	-0.060829	4.815448
299.372180	7999.971594	10.166874	-0.060823	4.815362
299.329556	8000.340733	10.171879	-0.060815	4.815470
299.445934	8000.004884	10.176883	-0.060836	4.815372
299.497195	8000.107281	10.181888	-0.060846	4.815401
299.434691	8000.085935	10.186893	-0.060834	4.815395
299.683304	8000.091127	10.191898	-0.060881	4.815396
299.572717	8000.109602	10.196903	-0.060860	4.815402
299.571940	8000.094624	10.201907	-0.060860	4.815397
299.281792	8000.029953	10.206912	-0.060806	4.815380
299.332777	8000.136621	10.211917	-0.060815	4.815411
299.578698	8000.169560	10.216922	-0.060861	4.815419
299.415595	8000.185027	10.221927	-0.060831	4.815424
299.503030	8000.102032	10.226931	-0.060847	4.815400
299.445102	8000.172689	10.231936	-0.060836	4.815421
299.459635	8000.222100	10.236941	-0.060839	4.815435
299.364205	8000.116832	10.241946	-0.060821	4.815405
299.510089	8000.175904	10.246951	-0.060848	4.815421
299.523177	8000.181466	10.251955	-0.060851	4.815423
299.510799	8000.195156	10.256960	-0.060849	4.815427
299.591468	8000.286284	10.261965	-0.060864	4.815453
299.810347	8000.103921	10.266970	-0.060904	4.815399
299.665480	8000.200928	10.271975	-0.060877	4.815428
299.608929	8000.162578	10.276979	-0.060867	4.815417
299.652994	8000.262719	10.281984	-0.060875	4.815446
299.515113	8000.092610	10.286989	-0.060849	4.815397
299.655885	8000.085325	10.291994	-0.060876	4.815394
299.782844	8000.274493	10.296999	-0.060899	4.815449
299.708700	8000.000687	10.302003	-0.060885	4.815369
299.734621	8000.127249	10.307008	-0.060890	4.815406
299.829852	8000.099968	10.312013	-0.060908	4.815398
299.780682	8000.221010	10.317018	-0.060899	4.815433
299.599685	8000.153872	10.322023	-0.060865	4.815414
299.786780	8000.010532	10.327027	-0.060900	4.815372
299.630203	8000.032521	10.332032	-0.060871	4.815379
299.517974	8000.318200	10.337037	-0.060850	4.815463
299.546544	7999.979825	10.342042	-0.060855	4.815364
299.569794	8000.181167	10.347047	-0.060860	4.815423
299.739644	8000.077092	10.352051	-0.060891	4.815391
299.560264	8000.079461	10.357056	-0.060858	4.815393
299.618459	7999.989568	10.362061	-0.060868	4.815366
299.768763	8000.110711	10.367066	-0.060897	4.815401
299.768143	8000.110701	10.372071	-0.060896	4.815401
299.856805	7999.961453	10.377075	-0.060913	4.815357
299.724629	8000.010569	10.382080	-0.060888	4.815372
299.616909	8000.085744	10.387085	-0.060868	4.815395
299.526587	8000.010491	10.392090	-0.060851	4.815373
299.626503	8000.051698	10.397095	-0.060870	4.815385
299.812591	8000.001338	10.402099	-0.060905	4.815369
299.744264	8000.011963	10.407104	-0.060892	4.815372
299.682239	8000.048346	10.412109	-0.060880	4.815383
299.946944	8000.021738	10.417114	-0.060930	4.815374
299.700014	8000.146982	10.422119	-0.060884	4.815412
299.525413	7999.951681	10.427123	-0.060851	4.815356
299.608327	8000.187148	10.432128	-0.060867	4.815424
299.653915	8000.024360	10.437133	-0.060875	4.815376
299.594760	8000.056515	10.442138	-0.060864	4.815386
299.460578	8000.349312	10.447143	-0.060839	4.815472
299.506958	8000.124538	10.452147	-0.060848	4.815406
299.538998	8000.269374	10.457152	-0.060854	4.815449
299.608421	8000.152944	10.462157	-0.060867	4.815414
299.846989	8000.004045	10.467162	-0.060911	4.815370
299.556101	8000.143524	10.472167	-0.060857	4.815412
299.393143	8000.124787	10.477171	-0.060827	4.815407
299.593924	7999.978469	10.482176	-0.060864	4.815363
299.631368	8000.151186	10.487181	-0.060871	4.815414
299.662345	7999.986017	10.492186	-0.060877	4.815365
299.706379	8000.154567	10.497191	-0.060885	4.815414
299.938540	8000.039768	10.502195	-0.060928	4.815380
299.954413	8000.133027	10.507200	-0.060931	4.815407
299.719440	8000.015824	10.512205	-0.060887	4.815374
299.889447	8000.038953	10.517210	-0.060919	4.815380
299.924029	8000.138937	10.522215	-0.060925	4.815409
299.635322	7999.954569	10.527219	-0.060872	4.815356
299.790210	8000.083270	10.532224	-0.060900	4.815393
299.804436	8000.055714	10.537229	-0.060903	4.815385
299.912144	8000.011537	10.542234	-0.060923	4.815371
299.805131	8000.146584	10.547239	-0.060903	4.815411
299.932422	7999.986219	10.552243	-0.060927	4.815364
299.933195	7999.977680	10.557248	-0.060927	4.815361
299.893628	8000.042228	10.562253	-0.060920	4.815380
300.033067	8000.056299	10.567258	-0.060946	4.815384
300.052503	8000.164583	10.572263	-0.060949	4.815415
299.760200	8000.139424	10.577267	-0.060895	4.815409
299.773479	8000.135368	10.582272	-0.060897	4.815408
299.756621	8000.111572	10.587277	-0.060894	4.815401
299.946680	8000.012108	10.592282	-0.060930	4.815371
300.048998	8000.092906	10.597287	-0.060949	4.815395
300.002852	7999.963869	10.602291	-0.060940	4.815357
299.852686	8000.249988	10.607296	-0.060912	4.815441
299.782333	8000.083137	10.612301	-0.060899	4.815393
299.857845	8000.030943	10.617306	-0.060913	4.815377
299.787642	8000.000918	10.622311	-0.060900	4.815369
299.965183	8000.132134	10.627315	-0.060933	4.815406
299.800096	7999.980815	10.632320	-0.060902	4.815363
299.969733	8000.154656	10.637325	-0.060934	4.815413
300.104060	8000.049992	10.642330	-0.060959	4.815382
299.931016	8000.120877	10.647335	-0.060927	4.815403
300.025004	7999.962097	10.652339	-0.060944	4.815356
300.088338	8000.020869	10.657344	-0.060956	4.815373
299.634049	8000.108468	10.662349	-0.060871	4.815401
299.820691	7999.967259	10.667354	-0.060906	4.815359
299.779508	8000.059572	10.672359	-0.060898	4.815386
299.885131	8000.012154	10.677363	-0.060918	4.815372
299.966862	8000.173848	10.682368	-0.060933	4.815419
299.915495	8000.001968	10.687373	-0.060924	4.815369
299.905179	8000.107620	10.692378	-0.060922	4.815399
299.782455	8000.083137	10.697383	-0.060899	4.815393
299.979557	8000.044718	10.702387	-0.060936	4.815381
300.016833	8000.085955	10.707392	-0.060943	4.815393
299.678548	8000.181892	10.712397	-0.060880	4.815422
299.818821	8000.129703	10.717402	-0.060906	4.815406
300.077643	8000.197064	10.722407	-0.060954	4.815425
300.031456	8000.042371	10.727411	-0.060945	4.815380
300.030454	8000.069078	10.732416	-0.060945	4.815388
299.910987	8000.094888	10.737421	-0.060923	4.815396
300.034266	8000.100140	10.742426	-0.060946	4.815397
300.170162	8000.078877	10.747431	-0.060971	4.815390
300.241119	8000.040504	10.752435	-0.060984	4.815378
300.071911	8000.085799	10.757440	-0.060953	4.815392
300.023448	8000.079650	10.762445	-0.060944	4.815391
300.057213	8000.001109	10.767450	-0.060950	4.815368
300.142339	8000.233411	10.772455	-0.060966	4.815435
300.013782	8000.244105	10.777459	-0.060942	4.815439
299.887289	8000.023944	10.782464	-0.060918	4.815375
299.902455	8000.049850	10.787469	-0.060921	4.815383
299.954498	8000.138365	10.792474	-0.060931	4.815408
300.097564	8000.066982	10.797479	-0.060958	4.815387
300.087494	8000.109572	10.802483	-0.060956	4.815399
299.989845	8000.144296	10.807488	-0.060938	4.815410
300.054740	8000.168889	10.812493	-0.060950	4.815417
300.134401	8000.128522	10.817498	-0.060964	4.815404
300.019571	8000.259165	10.822503	-0.060943	4.815443
300.128948	8000.119880	10.827507	-0.060963	4.815402
300.053902	8000.148565	10.832512	-0.060949	4.815411
300.094232	8000.133200	10.837517	-0.060957	4.815406
300.252911	7999.934873	10.842522	-0.060986	4.815347
300.136520	8000.144590	10.847527	-0.060965	4.815409
300.317563	8000.023597	10.852531	-0.060998	4.815373
300.223233	8000.060514	10.857536	-0.060981	4.815384
300.068509	8000.062223	10.862541	-0.060952	4.815385
300.111566	7999.903667	10.867546	-0.060960	4.815339
299.962025	8000.123523	10.872551	-0.060932	4.815404
300.145621	7999.961953	10.877555	-0.060966	4.815356
300.092289	8000.119270	10.882560	-0.060957	4.815402
300.081924	8000.066720	10.887565	-0.060955	4.815387
300.261976	7999.982054	10.892570	-0.060988	4.815361
300.027504	8000.155607	10.897575	-0.060945	4.815413
300.244438	8000.162413	10.902579	-0.060985	4.815414
300.357643	8000.067018	10.907584	-0.061006	4.815385
300.233003	8000.058536	10.912589	-0.060983	4.815384
300.258498	8000.089958	10.917594	-0.060988	4.815393
300.212617	8000.087059	10.922599	-0.060979	4.815392
300.410610	7999.996277	10.927603	-0.061016	4.815365
300.214495	8000.087090	10.932608	-0.060979	4.815392
300.293273	8000.119396	10.937613	-0.060994	4.815401
300.282073	7999.961008	10.942618	-0.060992	4.815355
300.221500	8000.046586	10.947623	-0.060981	4.815380
300.201551	7999.985326	10.952627	-0.060977	4.815362
300.135899	7999.972479	10.957632	-0.060965	4.815359
300.054398	8000.071606	10.962637	-0.060949	4.815388
300.168457	8000.084187	10.967642	-0.060971	4.815391
300.077132	8000.115809	10.972647	-0.060954	4.815401
300.267838	7999.981080	10.977651	-0.060989	4.815361
300.248293	8000.185992	10.982656	-0.060986	4.815421
300.265207	8000.191617	10.987661	-0.060989	4.815422
300.471964	7999.864746	10.992666	-0.061027	4.815326
300.013207	8000.136126	10.997671	-0.060942	4.815407
300.198502	8000.087892	11.002675	-0.060976	4.815392
300.264208	8000.097533	11.007680	-0.060989	4.815395
300.107092	8000.078892	11.012685	-0.060959	4.815390
300.177278	7999.976370	11.017690	-0.060972	4.815360
300.160911	8000.201644	11.022695	-0.060969	4.815426
300.300777	8000.168689	11.027699	-0.060995	4.815415
300.176758	8000.065082	11.032704	-0.060972	4.815386
300.281940	8000.001622	11.037709	-0.060992	4.815367
300.426888	8000.006164	11.042714	-0.061019	4.815367
300.391022	7999.978846	11.047719	-0.061012	4.815360
300.388800	7999.957430	11.052723	-0.061012	4.815353
300.192213	7999.988375	11.057728	-0.060975	4.815363
300.353239	8000.137490	11.062733	-0.061005	4.815406
300.143560	7999.971534	11.067738	-0.060966	4.815359
300.320637	8000.175431	11.072743	-0.060999	4.815417
300.544243	7999.930078	11.077747	-0.061041	4.815345
300.331317	8000.018474	11.082752	-0.061001	4.815371
300.251942	8000.266220	11.087757	-0.060986	4.815444
300.389558	7999.925374	11.092762	-0.061012	4.815344
300.384844	8000.121980	11.097767	-0.061011	4.815401
300.291836	8000.050955	11.102771	-0.060994	4.815381
300.247235	8000.146420	11.107776	-0.060985	4.815409
300.356604	8000.076615	11.112781	-0.061006	4.815388
300.369431	8000.082172	11.117786	-0.061008	4.815390
300.291953	8000.236952	11.122791	-0.060994	4.815435
300.410012	8000.176912	11.127795	-0.061016	4.815417
300.377203	8000.039544	11.132800	-0.061010	4.815377
300.191563	8000.079221	11.137805	-0.060975	4.815390
300.486222	7999.975078	11.142810	-0.061030	4.815358
300.499516	8000.004159	11.147815	-0.061032	4.815366
300.461536	7999.959703	11.152819	-0.061025	4.815354
300.545711	7999.977133	11.157824	-0.061041	4.815358
300.459970	8000.075122	11.162829	-0.061025	4.815387
300.396740	7999.887009	11.167834	-0.061013	4.815333
300.328517	8000.077216	11.172839	-0.061000	4.815389
300.383678	8000.150819	11.177843	-0.061011	4.815410
300.572446	8000.053471	11.182848	-0.061046	4.815380
300.436265	8000.071521	11.187853	-0.061021	4.815386
300.582743	7999.998056	11.192858	-0.061048	4.815364
300.431698	8000.228580	11.197863	-0.061020	4.815432
300.404173	8000.130849	11.202867	-0.061015	4.815404
300.398692	8000.157481	11.207872	-0.061014	4.815412
300.391807	8000.076127	11.212877	-0.061012	4.815388
300.495271	8000.039362	11.217882	-0.061031	4.815377
300.209326	8000.113719	11.222887	-0.060978	4.815400
300.315732	8000.089830	11.227891	-0.060998	4.815392
300.367311	8000.004102	11.232896	-0.061008	4.815367
300.277090	8000.176841	11.237901	-0.060991	4.815418
300.549478	7999.983607	11.242906	-0.061042	4.815360
300.431429	8000.195436	11.247911	-0.061020	4.815423
300.481870	8000.068000	11.252915	-0.061029	4.815385
300.489296	7999.999711	11.257920	-0.061030	4.815365
300.428192	8000.124832	11.262925	-0.061019	4.815402
300.598985	7999.953428	11.267930	-0.061051	4.815351
300.278873	8000.074252	11.272935	-0.060991	4.815388
300.378684	8000.085528	11.277939	-0.061010	4.815391
300.592383	7999.998214	11.282944	-0.061050	4.815364
300.427090	8000.002954	11.287949	-0.061019	4.815366
300.387583	8000.065366	11.292954	-0.061011	4.815385
300.381480	8000.037472	11.297959	-0.061010	4.815377
300.605906	8000.066850	11.302963	-0.061052	4.815384
300.668098	8000.047571	11.307968	-0.061064	4.815378
300.563065	8000.125999	11.312973	-0.061044	4.815402
300.473144	7999.943857	11.317978	-0.061027	4.815349
300.449452	8000.203216	11.322983	-0.061023	4.815425
300.656760	8000.003556	11.327987	-0.061061	4.815365
300.583549	8000.062202	11.332992	-0.061048	4.815383
300.459366	7999.983178	11.337997	-0.061025	4.815360
300.578559	7999.973397	11.343002	-0.061047	4.815357
300.726179	8000.142601	11.348007	-0.061074	4.815406
300.513836	8000.019356	11.353011	-0.061035	4.815371
300.689888	8000.037242	11.358016	-0.061068	4.815375
300.456258	8000.127433	11.363021	-0.061024	4.815403
300.376004	8000.027759	11.368026	-0.061009	4.815374
300.378860	8000.149665	11.373031	-0.061010	4.815409
300.476680	8000.086082	11.378035	-0.061028	4.815390
300.636681	8000.049186	11.383040	-0.061058	4.815379
300.393789	8000.121051	11.388045	-0.061013	4.815401
300.595846	8000.081645	11.393050	-0.061050	4.815389
300.584740	8000.188356	11.398055	-0.061048	4.815420
300.555838	8000.109843	11.403059	-0.061043	4.815397
300.504251	8000.098297	11.408064	-0.061033	4.815394
300.662675	8000.084891	11.413069	-0.061063	4.815389
300.743613	7999.964375	11.418074	-0.061078	4.815354
300.571580	8000.120793	11.423079	-0.061046	4.815400
300.594822	7999.980078	11.428083	-0.061050	4.815359
300.762456	7999.955067	11.433088	-0.061081	4.815351
300.716868	8000.115721	11.438093	-0.061073	4.815398
300.580956	7999.914643	11.443098	-0.061047	4.815340
300.536610	8000.064627	11.448103	-0.061039	4.815384
300.529770	7999.955482	11.453107	-0.061038	4.815352
300.586723	8000.048355	11.458112	-0.061048	4.815379
300.536991	8000.037909	11.463117	-0.061039	4.815376
300.579042	7999.934920	11.468122	-0.061047	4.815346
300.302529	8000.218946	11.473127	-0.060996	4.815430
300.332375	8000.017411	11.478131	-0.061001	4.815371
300.755777	8000.024435	11.483136	-0.061080	4.815371
300.498271	8000.012680	11.488141	-0.061032	4.815369
300.703277	8000.021426	11.493146	-0.061070	4.815370
300.560409	8000.078916	11.498151	-0.061044	4.815388
300.546840	8000.028451	11.503155	-0.061041	4.815373
300.473022	8000.095638	11.508160	-0.061027	4.815393
300.363985	7999.985867	11.513165	-0.061007	4.815362
300.688999	8000.071429	11.518170	-0.061067	4.815385
300.661168	8000.083794	11.523175	-0.061062	4.815389
300.606066	8000.103190	11.528179	-0.061052	4.815395
300.751089	7999.996564	11.533184	-0.061079	4.815363
300.680187	8000.046696	11.538189	-0.061066	4.815378
300.635720	7999.946547	11.543194	-0.061057	4.815349
300.714567	8000.011991	11.548199	-0.061072	4.815368
300.479957	8000.120338	11.553203	-0.061029	4.815400
300.458499	8000.010950	11.558208	-0.061025	4.815369
300.501995	8000.026636	11.563213	-0.061033	4.815373
300.422836	7999.943015	11.568218	-0.061018	4.815349
300.301831	8000.131278	11.573223	-0.060995	4.815404
300.520605	8000.001290	11.578227	-0.061036	4.815365
300.573771	8000.001103	11.583232	-0.061046	4.815365
300.626814	8000.088567	11.588237	-0.061056	4.815390
300.636092	7999.940138	11.593242	-0.061058	4.815347
300.650648	8000.200133	11.598247	-0.061060	4.815423
300.797347	7999.973812	11.603251	-0.061088	4.815356
300.628001	8000.118517	11.608256	-0.061056	4.815399
300.578733	8000.027908	11.613261	-0.061047	4.815373
300.562893	8000.065058	11.618266	-0.061044	4.815384
300.455895	7999.986319	11.623271	-0.061024	4.815361
300.374256	8000.117513	11.628275	-0.061009	4.815400
300.581257	8000.110258	11.633280	-0.061047	4.815397
300.561222	8000.133442	11.638285	-0.061044	4.815404
300.621812	8000.025415	11.643290	-0.061055	4.815372
300.593693	8000.045258	11.648295	-0.061050	4.815378
300.580809	8000.098491	11.653299	-0.061047	4.815394
300.791945	7999.912792	11.658304	-0.061086	4.815338
300.715463	8000.105001	11.663309	-0.061072	4.815395
300.808474	7999.895963	11.668314	-0.061090	4.815333
300.776684	8000.029053	11.673319	-0.061084	4.815372
300.610107	8000.108597	11.678323	-0.061053	4.815396
300.601624	8000.087078	11.683328	-0.061051	4.815390
300.915609	8000.179942	11.688333	-0.061110	4.815416
300.604048	8000.088186	11.693338	-0.061052	4.815390
300.597096	8000.093416	11.698343	-0.061050	4.815392
300.773278	8000.178648	11.703347	-0.061083	4.815416
300.688454	8000.007278	11.708352	-0.061067	4.815366
300.494812	8000.117373	11.713357	-0.061031	4.815399
300.579298	7999.963778	11.718362	-0.061047	4.815354
300.573978	8000.004309	11.723367	-0.061046	4.815366
300.506425	7999.965776	11.728371	-0.061033	4.815355
300.482340	8000.067994	11.733376	-0.061029	4.815385
300.587293	8000.069735	11.738381	-0.061048	4.815385
300.634699	8000.001040	11.743386	-0.061057	4.815365
300.611864	8000.030592	11.748391	-0.061053	4.815374
300.555056	8000.103406	11.753395	-0.061042	4.815395
300.615377	8000.027443	11.758400	-0.061054	4.815373
300.487523	8000.069148	11.763405	-0.061030	4.815385
300.648197	7999.989505	11.768410	-0.061060	4.815361
300.653640	8000.023801	11.773415	-0.061061	4.815371
300.406384	8000.040009	11.778419	-0.061015	4.815377
300.530102	8000.212024	11.783424	-0.061038	4.815427
300.789470	8000.250535	11.788429	-0.061086	4.815437
300.795702	8000.111674	11.793434	-0.061087	4.815396
300.635836	8000.122917	11.798439	-0.061058	4.815400
300.572523	8000.107970	11.803443	-0.061046	4.815396
300.790736	8000.070971	11.808448	-0.061086	4.815385
300.521947	8000.071855	11.813453	-0.061036	4.815386
300.568492	7999.964665	11.818458	-0.061045	4.815355
300.721419	7999.987512	11.823463	-0.061073	4.815360
300.680190	7999.965449	11.828467	-0.061066	4.815354
300.774725	7999.994809	11.833472	-0.061083	4.815362
300.781354	8000.124262	11.838477	-0.061085	4.815400
300.657182	7999.959722	11.843482	-0.061061	4.815353
300.633127	8000.075837	11.848487	-0.061057	4.815387
300.581723	8000.131638	11.853491	-0.061047	4.815403
300.776729	8000.145563	11.858496	-0.061084	4.815406
300.693530	8000.108907	11.863501	-0.061068	4.815396
300.857597	7999.957701	11.868506	-0.061099	4.815351
300.893395	8000.061983	11.873511	-0.061105	4.815381
300.792460	8000.069928	11.878515	-0.061087	4.815384
300.726138	8000.016450	11.883520	-0.061074	4.815369
300.752411	8000.222124	11.888525	-0.061079	4.815429
300.692957	8000.055450	11.893530	-0.061068	4.815380
300.607474	8000.191925	11.898535	-0.061052	4.815421
300.565081	8000.075775	11.903539	-0.061044	4.815387
300.905555	8000.138079	11.908544	-0.061108	4.815404
300.705166	8000.147581	11.913549	-0.061070	4.815407
300.611914	8000.213377	11.918554	-0.061053	4.815427
300.724318	8000.024970	11.923559	-0.061074	4.815371
300.890433	8000.179517	11.928563	-0.061105	4.815416
300.820710	7999.967777	11.933568	-0.061092	4.815354
300.735362	8000.200460	11.938573	-0.061076	4.815423
300.686195	8000.066025	11.943578	-0.061067	4.815384
300.838688	8000.070693	11.948583	-0.061095	4.815384
300.734430	8000.189755	11.953587	-0.061076	4.815419
300.775953	8000.012998	11.958592	-0.061083	4.815368
300.647175	8000.184031	11.963597	-0.061060	4.815418
300.780461	8000.137071	11.968602	-0.061084	4.815404
300.834731	8000.083454	11.973607	-0.061094	4.815388
300.600593	8000.154395	11.978611	-0.061051	4.815410
300.819659	8000.113135	11.983616	-0.061092	4.815397
300.537899	8000.167251	11.988621	-0.061039	4.815414
300.691241	8000.168727	11.993626	-0.061068	4.815414
300.425379	8000.201728	11.998631	-0.061018	4.815424
300.803841	8000.158837	12.003635	-0.061089	4.815410
300.917185	8000.083753	12.008640	-0.061110	4.815388
300.713229	8000.146643	12.013645	-0.061072	4.815407
300.808078	8000.116148	12.018650	-0.061090	4.815398
300.737621	8000.098945	12.023655	-0.061076	4.815393
300.853138	7999.979002	12.028659	-0.061098	4.815357
300.750628	7999.995473	12.033664	-0.061079	4.815363
300.839534	8000.120946	12.038669	-0.061095	4.815399
300.824442	8000.213694	12.043674	-0.061093	4.815426
300.868802	8000.154569	12.048679	-0.061101	4.815409
300.672578	8000.276380	12.053683	-0.061064	4.815445
300.930890	8000.070082	12.058688	-0.061112	4.815384
300.934398	8000.155657	12.063693	-0.061113	4.815409
300.861849	8000.010144	12.068698	-0.061099	4.815366
300.795797	8000.119150	12.073703	-0.061087	4.815399
300.735879	8000.204740	12.078707	-0.061076	4.815424
300.737931	8000.017708	12.083712	-0.061076	4.815369
300.728187	8000.206750	12.088717	-0.061075	4.815424
300.981055	7999.991812	12.093722	-0.061122	4.815360
300.889790	8000.163467	12.098727	-0.061105	4.815411
301.040367	7999.952175	12.103731	-0.061133	4.815349
301.001746	8000.075533	12.108736	-0.061126	4.815385
300.963706	8000.108039	12.113741	-0.061118	4.815395
300.837068	8000.086696	12.118746	-0.061095	4.815389
300.938548	8000.062725	12.123751	-0.061114	4.815381
300.901754	8000.105941	12.128755	-0.061107	4.815394
300.827750	8000.106851	12.133760	-0.061093	4.815395
300.737671	8000.089322	12.138765	-0.061076	4.815390
300.935413	8000.062672	12.143770	-0.061113	4.815381
300.943760	8000.053190	12.148775	-0.061115	4.815379
300.872244	8000.286105	12.153779	-0.061102	4.815447
300.881994	8000.167612	12.158784	-0.061103	4.815412
300.859066	8000.104163	12.163789	-0.061099	4.815394
301.119392	8000.130931	12.168794	-0.061147	4.815400
301.086371	8000.151762	12.173799	-0.061141	4.815407
301.008302	8000.108777	12.178803	-0.061127	4.815395
300.938990	7999.974008	12.183808	-0.061114	4.815355
300.757533	8000.247855	12.188813	-0.061080	4.815436
300.859317	8000.077442	12.193818	-0.061099	4.815386
300.963686	8000.096277	12.198823	-0.061118	4.815391
300.897533	8000.077007	12.203827	-0.061106	4.815386
300.850540	7999.980022	12.208832	-0.061097	4.815358
300.822103	8000.240374	12.213837	-0.061092	4.815434
300.850401	8000.129672	12.218842	-0.061097	4.815401
300.888238	8000.152748	12.223847	-0.061104	4.815408
300.937485	8000.096911	12.228851	-0.061114	4.815391
301.003697	8000.119388	12.233856	-0.061126	4.815398
300.783944	8000.159569	12.238861	-0.061085	4.815410
300.885664	8000.097119	12.243866	-0.061104	4.815392
301.015089	8000.090715	12.248871	-0.061128	4.815389
301.003358	8000.091589	12.253875	-0.061126	4.815390
301.172179	8000.086908	12.258880	-0.061157	4.815387
301.031892	8000.087787	12.263885	-0.061131	4.815388
300.904674	7999.985194	12.268890	-0.061107	4.815359
300.766592	8000.014972	12.273895	-0.061082	4.815368
301.011855	8000.213591	12.278899	-0.061127	4.815425
301.044483	8000.011031	12.283904	-0.061133	4.815366
300.871855	8000.172785	12.288909	-0.061101	4.815414
300.855457	8000.129754	12.293914	-0.061098	4.815401
301.014398	8000.155909	12.298919	-0.061128	4.815408
300.895465	8000.111177	12.303923	-0.061106	4.815396
300.961718	7999.972243	12.308928	-0.061118	4.815355
300.962603	8000.126187	12.313933	-0.061118	4.815400
300.962675	7999.935915	12.318938	-0.061118	4.815344
300.875265	8000.024256	12.323943	-0.061102	4.815370
300.968897	8000.139118	12.328947	-0.061119	4.815404
301.123415	8000.134200	12.333952	-0.061148	4.815401
300.710633	8000.099557	12.338957	-0.061071	4.815393
300.716416	7999.984207	12.343962	-0.061072	4.815360
300.928533	8000.184413	12.348967	-0.061112	4.815417
300.721800	8000.179913	12.353971	-0.061073	4.815417
301.046425	8000.084818	12.358976	-0.061134	4.815387
300.947469	7999.976281	12.363981	-0.061115	4.815356
300.973495	8000.028022	12.368986	-0.061120	4.815371
300.738960	8000.212266	12.373991	-0.061077	4.815426
300.787643	8000.123281	12.378995	-0.061086	4.815400
300.995557	8000.094663	12.384000	-0.061124	4.815390
301.049785	8000.180011	12.389005	-0.061134	4.815415
301.062073	8000.197318	12.394010	-0.061137	4.815420
300.831063	8000.130415	12.399015	-0.061094	4.815402
300.723706	8000.071979	12.404019	-0.061074	4.815385
300.774697	8000.041826	12.409024	-0.061083	4.815376
300.913299	8000.168124	12.414029	-0.061109	4.815412
300.874921	8000.042420	12.419034	-0.061102	4.815376
300.975107	8000.036599	12.424039	-0.061120	4.815374
301.059185	8000.089304	12.429043	-0.061136	4.815389
301.196921	7999.998591	12.434048	-0.061162	4.815361
301.005125	8000.098027	12.439053	-0.061126	4.815391
300.853267	8000.119024	12.444058	-0.061098	4.815398
301.073822	7999.936686	12.449063	-0.061139	4.815344
300.852128	8000.105108	12.454067	-0.061098	4.815394
300.932036	7999.979229	12.459072	-0.061112	4.815357
300.960933	8000.124017	12.464077	-0.061118	4.815399
301.014926	8000.029776	12.469082	-0.061128	4.815371
300.974494	8000.116759	12.474087	-0.061120	4.815397
301.044164	8000.109363	12.479091	-0.061133	4.815395
300.998560	8000.019883	12.484096	-0.061125	4.815369
300.990897	8000.280582	12.489101	-0.061124	4.815445
300.986639	8000.062443	12.494106	-0.061123	4.815381
301.139712	8000.006191	12.499111	-0.061151	4.815364
301.001510	8000.137517	12.504115	-0.061125	4.815403
301.092007	8000.152915	12.509120	-0.061142	4.815407
301.228306	8000.150901	12.514125	-0.061168	4.815406
301.062863	8000.033777	12.519130	-0.061137	4.815372
301.138506	8000.018998	12.524135	-0.061151	4.815368
301.060291	8000.002734	12.529139	-0.061136	4.815363
301.216399	7999.977532	12.534144	-0.061165	4.815355
301.061921	8000.110725	12.539149	-0.061137	4.815395
301.059471	7999.944997	12.544154	-0.061136	4.815346
301.174753	7999.944772	12.549159	-0.061158	4.815346
301.110150	8000.126491	12.554163	-0.061146	4.815399
301.004877	8000.011434	12.559168	-0.061126	4.815366
301.073492	8000.223158	12.564173	-0.061139	4.815428
301.125796	7999.959993	12.569178	-0.061148	4.815350
301.025778	8000.102642	12.574183	-0.061130	4.815393
300.943233	8000.095927	12.579187	-0.061114	4.815391
300.860385	8000.048587	12.584192	-0.061099	4.815378
300.964295	8000.288689	12.589197	-0.061119	4.815447
300.831133	8000.072687	12.594202	-0.061094	4.815385
301.071442	8000.175019	12.599207	-0.061138	4.815414
301.007736	8000.175031	12.604211	-0.061127	4.815414
301.221099	7999.944470	12.609216	-0.061166	4.815345
301.057838	8000.161965	12.614221	-0.061136	4.815410
301.046657	7999.983264	12.619226	-0.061134	4.815358
301.216541	7999.951877	12.624231	-0.061165	4.815348
301.002364	7999.985736	12.629235	-0.061125	4.815359
301.305687	7999.966183	12.634240	-0.061182	4.815351
301.165281	8000.158403	12.639245	-0.061156	4.815408
301.273782	8000.014825	12.644250	-0.061176	4.815366
301.265846	8000.084176	12.649255	-0.061175	4.815386
301.245514	8000.094528	12.654259	-0.061171	4.815389
301.235284	8000.048393	12.659264	-0.061169	4.815376
301.274083	8000.208312	12.664269	-0.061176	4.815422
301.346372	8000.156063	12.669274	-0.061190	4.815407
301.399002	7999.986972	12.674279	-0.061199	4.815357
301.173423	8000.105089	12.679283	-0.061157	4.815393
301.164491	8000.017286	12.684288	-0.061156	4.815367
301.071161	8000.157909	12.689293	-0.061138	4.815409
301.060859	8000.154531	12.694298	-0.061136	4.815408
301.213666	7999.979620	12.699303	-0.061165	4.815356
301.157101	8000.147576	12.704307	-0.061154	4.815405
301.069320	7999.975086	12.709312	-0.061138	4.815355
301.039330	8000.177690	12.714317	-0.061132	4.815414
301.137828	8000.122670	12.719322	-0.061151	4.815398
301.046342	8000.013187	12.724327	-0.061134	4.815366
301.000102	8000.120383	12.729331	-0.061125	4.815398
301.224554	8000.067454	12.734336	-0.061167	4.815381
301.237968	8000.032401	12.739341	-0.061169	4.815371
301.148616	8000.121779	12.744346	-0.061153	4.815398
301.346556	8000.083375	12.749351	-0.061190	4.815385
301.320398	8000.194113	12.754355	-0.061185	4.815418
301.256790	8000.069057	12.759360	-0.061173	4.815382
301.287640	8000.232051	12.764365	-0.061179	4.815429
301.336217	8000.083202	12.769370	-0.061188	4.815385
301.117213	8000.081705	12.774375	-0.061147	4.815386
300.979973	8000.102945	12.779379	-0.061121	4.815393
301.133641	8000.108702	12.784384	-0.061150	4.815394
301.245248	8000.125519	12.789389	-0.061171	4.815398
301.172392	8000.149965	12.794394	-0.061157	4.815406
301.093036	8000.048166	12.799399	-0.061142	4.815376
301.129312	8000.008147	12.804403	-0.061149	4.815365
301.239183	7999.997143	12.809408	-0.061169	4.815361
301.163415	8000.082471	12.814413	-0.061155	4.815386
301.276594	8000.189108	12.819418	-0.061177	4.815417
301.409769	8000.084422	12.824423	-0.061201	4.815385
301.249079	8000.338307	12.829427	-0.061172	4.815460
301.276257	7999.941103	12.834432	-0.061176	4.815344
301.231421	8000.148806	12.839437	-0.061168	4.815405
301.170099	8000.103960	12.844442	-0.061157	4.815392
301.288405	8000.055682	12.849447	-0.061179	4.815378
301.094311	8000.325047	12.854451	-0.061143	4.815457
301.108458	8000.080489	12.859456	-0.061145	4.815386
300.931118	8000.196200	12.864461	-0.061112	4.815420
301.238494	8000.291095	12.869466	-0.061169	4.815447
301.399602	8000.237114	12.874471	-0.061199	4.815430
301.223149	8000.286564	12.879475	-0.061167	4.815445
301.302133	8000.028116	12.884480	-0.061181	4.815370
301.507263	8000.173693	12.889485	-0.061219	4.815411
301.337273	8000.015872	12.894490	-0.061188	4.815366
301.330924	8000.163283	12.899495	-0.061187	4.815409
301.346965	8000.028860	12.904499	-0.061190	4.815370
301.251467	8000.055068	12.909504	-0.061172	4.815378
301.213599	8000.090784	12.914509	-0.061165	4.815388
301.370239	8000.183177	12.919514	-0.061194	4.815414
301.362512	8000.095393	12.924519	-0.061192	4.815389
301.224729	8000.174347	12.929523	-0.061167	4.815413
301.416962	8000.000090	12.934528	-0.061203	4.815361
301.223313	8000.247013	12.939533	-0.061167	4.815434
301.186538	8000.097816	12.944538	-0.061160	4.815390
301.369026	8000.035638	12.949543	-0.061194	4.815371
301.334223	8000.153716	12.954547	-0.061187	4.815406
301.321496	7999.982470	12.959552	-0.061185	4.815356
301.057595	8000.248537	12.964557	-0.061136	4.815435
301.166866	8000.071834	12.969562	-0.061156	4.815383
301.189707	8000.008076	12.974567	-0.061160	4.815364
301.191719	8000.379040	12.979571	-0.061161	4.815473
301.378683	8000.048625	12.984576	-0.061195	4.815375
301.517972	8000.217696	12.989581	-0.061221	4.815424
301.586104	8000.036033	12.994586	-0.061234	4.815370
301.602246	8000.119680	12.999591	-0.061237	4.815395
301.522605	8000.099117	13.004595	-0.061222	4.815389
301.496687	8000.059135	13.009600	-0.061217	4.815378
301.543112	8000.143285	13.014605	-0.061226	4.815402
301.474796	8000.083357	13.019610	-0.061213	4.815385
301.567912	8000.061385	13.024615	-0.061231	4.815378
301.403798	8000.036213	13.029619	-0.061200	4.815371
301.460567	7999.934535	13.034624	-0.061211	4.815341
301.502921	7999.932031	13.039629	-0.061218	4.815340
301.277997	8000.042677	13.044634	-0.061177	4.815374
301.248467	7999.979118	13.049639	-0.061171	4.815355
301.312178	7999.989796	13.054643	-0.061183	4.815358
301.363948	7999.954310	13.059648	-0.061193	4.815348
301.318700	8000.114972	13.064653	-0.061184	4.815395
301.166086	8000.015164	13.069658	-0.061156	4.815366
301.448863	8000.064753	13.074663	-0.061208	4.815380
301.471772	8000.131409	13.079667	-0.061213	4.815399
301.547748	7999.976601	13.084672	-0.061227	4.815353
301.353211	8000.005441	13.089677	-0.061191	4.815363
301.476304	8000.206312	13.094682	-0.061214	4.815421
301.465224	7999.983783	13.099687	-0.061211	4.815356
301.506238	8000.251705	13.104691	-0.061219	4.815434
301.517100	7999.965402	13.109696	-0.061221	4.815350
301.477858	8000.101578	13.114701	-0.061214	4.815390
301.488570	7999.962790	13.119706	-0.061216	4.815350
301.553154	7999.978827	13.124711	-0.061228	4.815354
301.405001	7999.989196	13.129715	-0.061200	4.815358
301.425503	8000.002364	13.134720	-0.061204	4.815361
301.473538	7999.986057	13.139725	-0.061213	4.815356
301.562283	8000.090151	13.144730	-0.061230	4.815386
301.597085	8000.104625	13.149735	-0.061236	4.815390
301.309056	8000.085947	13.154739	-0.061182	4.815386
301.369407	8000.076259	13.159744	-0.061194	4.815383
301.266388	8000.223135	13.164749	-0.061175	4.815427
301.303386	8000.051646	13.169754	-0.061181	4.815376
301.471163	8000.045879	13.174759	-0.061213	4.815374
301.232623	8000.139195	13.179763	-0.061168	4.815402
301.327985	8000.059537	13.184768	-0.061186	4.815379
301.453502	8000.173861	13.189773	-0.061209	4.815411
301.586378	8000.304344	13.194778	-0.061234	4.815449
301.625112	7999.988571	13.199783	-0.061241	4.815356
301.417774	8000.217095	13.204787	-0.061203	4.815424
301.553216	7999.988447	13.209792	-0.061228	4.815357
301.464893	8000.135567	13.214797	-0.061211	4.815400
301.451732	8000.140693	13.219802	-0.061209	4.815402
301.644792	7999.977139	13.224807	-0.061245	4.815353
301.559688	8000.058036	13.229811	-0.061229	4.815377
301.576264	7999.980277	13.234816	-0.061232	4.815354
301.447848	7999.912939	13.239821	-0.061208	4.815335
301.443568	7999.963109	13.244826	-0.061207	4.815350
301.408694	7999.989254	13.249831	-0.061201	4.815358
301.364030	8000.005616	13.254835	-0.061193	4.815363
301.470959	7999.974253	13.259840	-0.061212	4.815353
301.393152	7999.976168	13.264845	-0.061198	4.815354
301.440360	8000.106296	13.269850	-0.061207	4.815392
301.460061	8000.056381	13.274855	-0.061210	4.815377
301.486746	8000.241756	13.279859	-0.061216	4.815431
301.536902	7999.978553	13.284864	-0.061225	4.815354
301.328759	8000.167512	13.289869	-0.061186	4.815410
301.440871	8000.025062	13.294874	-0.061207	4.815368
301.582814	7999.990004	13.299879	-0.061233	4.815357
301.436798	8000.145787	13.304883	-0.061206	4.815403
301.532212	8000.088578	13.309888	-0.061224	4.815386
301.673257	8000.003264	13.314893	-0.061250	4.815360
301.545481	7999.977626	13.319898	-0.061226	4.815354
301.749922	7999.915812	13.324903	-0.061264	4.815335
301.768946	8000.081817	13.329907	-0.061268	4.815383
301.721187	7999.934576	13.334912	-0.061259	4.815340
301.757527	8000.003593	13.339917	-0.061266	4.815360
301.611099	8000.037507	13.344922	-0.061239	4.815371
301.600098	7999.964635	13.349927	-0.061236	4.815350
301.330871	8000.053166	13.354931	-0.061186	4.815377
301.602645	8000.065159	13.359936	-0.061237	4.815379
301.509299	7999.985575	13.364941	-0.061220	4.815356
301.491255	8000.165931	13.369946	-0.061216	4.815409
301.676576	7999.938110	13.374951	-0.061251	4.815341
301.639464	7999.997356	13.379955	-0.061244	4.815359
301.784023	8000.015790	13.384960	-0.061271	4.815364
301.410110	8000.036308	13.389965	-0.061201	4.815371
301.503218	8000.106267	13.394970	-0.061218	4.815391
301.611206	7999.974438	13.399975	-0.061239	4.815352
301.436370	7999.981157	13.404979	-0.061206	4.815355
301.643420	8000.064766	13.409984	-0.061245	4.815379
301.717498	8000.189996	13.414989	-0.061258	4.815415
301.557511	8000.070822	13.419994	-0.061229	4.815381
301.583021	8000.053073	13.424999	-0.061233	4.815375
301.495588	8000.155311	13.430003	-0.061217	4.815406
301.629736	8000.027124	13.435008	-0.061242	4.815368
301.509427	8000.181196	13.440013	-0.061220	4.815413
301.527609	8000.265947	13.445018	-0.061223	4.815438
301.534312	8000.067229	13.450023	-0.061224	4.815380
301.373820	8000.017531	13.455027	-0.061194	4.815366
301.709392	8000.170619	13.460032	-0.061257	4.815409
301.699225	8000.211071	13.465037	-0.061255	4.815421
301.622028	8000.083650	13.470042	-0.061241	4.815384
301.358059	8000.136993	13.475047	-0.061191	4.815401
301.336283	8000.140907	13.480051	-0.061187	4.815402
301.539811	8000.018147	13.485056	-0.061225	4.815365
301.537956	8000.034151	13.490061	-0.061225	4.815370
301.580606	8000.111824	13.495066	-0.061233	4.815393
301.567647	8000.014333	13.500071	-0.061230	4.815364
301.459343	8000.203880	13.505075	-0.061210	4.815420
301.531969	8000.122775	13.510080	-0.061224	4.815396
301.809900	8000.112423	13.515085	-0.061276	4.815392
301.620019	8000.135995	13.520090	-0.061240	4.815399
301.538395	7999.971088	13.525095	-0.061225	4.815352
301.520870	8000.137556	13.530099	-0.061222	4.815400
301.449493	7999.941820	13.535104	-0.061208	4.815344
301.716323	8000.026420	13.540109	-0.061258	4.815367
301.536768	8000.093991	13.545114	-0.061225	4.815388
301.590708	7999.977301	13.550119	-0.061235	4.815353
301.477981	8000.120809	13.555123	-0.061214	4.815396
301.461920	7999.974094	13.560128	-0.061211	4.815353
301.610307	8000.028936	13.565133	-0.061238	4.815368
301.462405	7999.997619	13.570138	-0.061211	4.815360
301.551468	7999.936028	13.575143	-0.061227	4.815341
301.554302	8000.109247	13.580147	-0.061228	4.815392
301.606271	8000.144317	13.585152	-0.061238	4.815402
301.478761	8000.192441	13.590157	-0.061214	4.815417
301.363593	7999.992771	13.595162	-0.061192	4.815359
301.680894	8000.073934	13.600167	-0.061251	4.815381
301.498449	7999.964009	13.605171	-0.061217	4.815350
301.606280	7999.944419	13.610176	-0.061238	4.815344
301.680179	8000.083542	13.615181	-0.061251	4.815384
301.368307	8000.080503	13.620186	-0.061193	4.815385
301.399198	8000.097051	13.625191	-0.061199	4.815389
301.610746	8000.152941	13.630195	-0.061238	4.815404
301.649384	8000.014617	13.635200	-0.061246	4.815364
301.642338	7999.986707	13.640205	-0.061244	4.815356
301.636460	8000.111678	13.645210	-0.061243	4.815392
301.648519	8000.014602	13.650215	-0.061245	4.815364
301.580304	8000.157780	13.655219	-0.061233	4.815406
301.520981	7999.931244	13.660224	-0.061222	4.815340
301.672976	7999.980801	13.665229	-0.061250	4.815354
301.642843	8000.007024	13.670234	-0.061244	4.815362
301.604646	8000.009597	13.675239	-0.061237	4.815363
301.581242	8000.059450	13.680243	-0.061233	4.815377
301.655089	8000.063882	13.685248	-0.061247	4.815378
301.485263	8000.113443	13.690253	-0.061215	4.815394
301.595288	8000.163373	13.695258	-0.061236	4.815408
301.623678	8000.063361	13.700263	-0.061241	4.815378
301.492913	8000.143500	13.705267	-0.061217	4.815402
301.545977	7999.955174	13.710272	-0.061226	4.815347
301.636590	8000.079609	13.715277	-0.061243	4.815383
301.673581	7999.947671	13.720282	-0.061250	4.815344
301.626072	7999.990710	13.725287	-0.061241	4.815357
301.485516	8000.001205	13.730291	-0.061215	4.815361
301.791511	8000.004145	13.735296	-0.061272	4.815360
301.859111	7999.989233	13.740301	-0.061285	4.815355
301.699533	8000.075308	13.745306	-0.061255	4.815381
301.819254	7999.989640	13.750311	-0.061277	4.815356
301.792276	7999.982778	13.755315	-0.061272	4.815354
301.567640	8000.078463	13.760320	-0.061230	4.815383
301.606453	7999.994659	13.765325	-0.061238	4.815358
301.708719	8000.097908	13.770330	-0.061257	4.815388
301.605924	7999.971133	13.775335	-0.061237	4.815351
301.781856	7999.993294	13.780339	-0.061270	4.815357
301.673125	8000.237353	13.785344	-0.061250	4.815429
301.674796	8000.189276	13.790349	-0.061250	4.815415
301.652937	7999.969775	13.795354	-0.061246	4.815351
301.916939	7999.972018	13.800359	-0.061295	4.815350
301.784014	8000.085261	13.805363	-0.061271	4.815384
301.552102	7999.976652	13.810368	-0.061227	4.815353
301.642748	7999.986708	13.815373	-0.061244	4.815356
301.570689	8000.135167	13.820378	-0.061231	4.815399
301.623896	8000.085809	13.825383	-0.061241	4.815385
301.542672	7999.986116	13.830387	-0.061226	4.815356
301.619318	8000.014112	13.835392	-0.061240	4.815364
301.741628	8000.026831	13.840397	-0.061263	4.815367
301.625963	8000.074084	13.845402	-0.061241	4.815381
301.671124	8000.048109	13.850407	-0.061250	4.815374
301.617725	7999.977740	13.855411	-0.061240	4.815353
301.686508	7999.999192	13.860416	-0.061252	4.815359
301.659800	8000.147335	13.865421	-0.061248	4.815403
301.759861	8000.139375	13.870426	-0.061266	4.815400
301.750495	8000.070805	13.875431	-0.061264	4.815380
301.555929	8000.138128	13.880435	-0.061228	4.815400
301.670964	7999.954037	13.885440	-0.061249	4.815346
301.757299	8000.050607	13.890445	-0.061266	4.815374
301.611489	8000.065291	13.895450	-0.061238	4.815379
301.780590	7999.957994	13.900455	-0.061270	4.815347
301.777040	7999.994279	13.905459	-0.061269	4.815357
301.694121	8000.019627	13.910464	-0.061254	4.815365
301.774700	8000.024171	13.915469	-0.061269	4.815366
301.831208	8000.281664	13.920474	-0.061280	4.815441
301.868808	7999.893181	13.925479	-0.061286	4.815327
301.844518	8000.121537	13.930483	-0.061282	4.815394
301.987730	7999.978534	13.935488	-0.061308	4.815352
301.867790	7999.951957	13.940493	-0.061286	4.815345
301.724810	8000.056480	13.945498	-0.061260	4.815376
301.959590	7999.919273	13.950503	-0.061303	4.815335
301.819005	8000.058044	13.955507	-0.061277	4.815376
301.537382	7999.930438	13.960512	-0.061225	4.815340
301.645281	8000.160988	13.965517	-0.061245	4.815407
301.728057	8000.069361	13.970522	-0.061260	4.815380
301.948586	8000.096539	13.975527	-0.061301	4.815386
301.876053	8000.133818	13.980531	-0.061288	4.815398
301.989156	8000.007419	13.985536	-0.061309	4.815360
301.994846	7999.933754	13.990541	-0.061310	4.815339
301.784734	7999.944163	13.995546	-0.061271	4.815343
301.667819	7999.951843	14.000551	-0.061249	4.815345
301.730146	8000.103602	14.005555	-0.061261	4.815390
301.790059	7999.994492	14.010560	-0.061272	4.815357
301.784428	8000.033951	14.015565	-0.061271	4.815369
301.666211	8000.009540	14.020570	-0.061249	4.815362
301.849129	8000.071369	14.025575	-0.061283	4.815380
301.714670	8000.016758	14.030579	-0.061258	4.815364
301.645526	7999.983541	14.035584	-0.061245	4.815355
301.589717	7999.965511	14.040589	-0.061234	4.815350
301.682702	8000.070744	14.045594	-0.061252	4.815380
301.731703	7999.958247	14.050599	-0.061261	4.815347
301.997916	7999.972286	14.055603	-0.061310	4.815350
301.968659	8000.092594	14.060608	-0.061305	4.815385
301.998802	8000.061025	14.065613	-0.061311	4.815376
301.830365	7999.975918	14.070618	-0.061279	4.815352
302.040708	7999.979410	14.075623	-0.061318	4.815352
301.920582	8000.103554	14.080627	-0.061296	4.815389
301.977243	8000.032873	14.085632	-0.061306	4.815368
302.103655	7999.966557	14.090637	-0.061330	4.815348
301.906413	8000.004973	14.095642	-0.061293	4.815360
301.891455	7999.894621	14.100647	-0.061290	4.815328
301.722738	8000.046821	14.105651	-0.061259	4.815373
301.952923	7999.875331	14.110656	-0.061302	4.815322
301.833329	7999.989863	14.115661	-0.061280	4.815356
301.753459	7999.959675	14.120666	-0.061265	4.815347
301.905548	7999.832854	14.125671	-0.061293	4.815310
301.670179	8000.113293	14.130675	-0.061249	4.815393
301.601581	7999.961430	14.135680	-0.061236	4.815349
301.736616	8000.096223	14.140685	-0.061262	4.815387
301.778064	8000.068048	14.145690	-0.061269	4.815379
301.720608	7999.914232	14.150695	-0.061259	4.815334
302.010373	8000.123216	14.155699	-0.061313	4.815394
301.847785	8000.036067	14.160704	-0.061282	4.815369
301.977416	8000.053185	14.165709	-0.061307	4.815374
301.908198	8000.153588	14.170714	-0.061294	4.815403
301.903959	8000.087241	14.175719	-0.061293	4.815384
301.826511	8000.053886	14.180723	-0.061278	4.815375
301.728020	8000.112113	14.185728	-0.061260	4.815392
301.856950	7999.954977	14.190733	-0.061284	4.815345
301.614942	8000.073891	14.195738	-0.061239	4.815381
301.687946	8000.026999	14.200743	-0.061253	4.815367
301.708250	8000.126750	14.205747	-0.061256	4.815396
301.809168	7999.963804	14.210752	-0.061275	4.815348
301.893134	7999.891439	14.215757	-0.061291	4.815327
301.921787	7999.993466	14.220762	-0.061296	4.815356
301.822510	7999.894542	14.225767	-0.061278	4.815328
301.761955	7999.967295	14.230771	-0.061266	4.815350
301.916739	8000.021175	14.235776	-0.061295	4.815365
302.033095	7999.931175	14.240781	-0.061317	4.815338
301.786869	8000.064985	14.245786	-0.061271	4.815378
301.811106	8000.058973	14.250791	-0.061276	4.815376
301.796897	8000.011702	14.255795	-0.061273	4.815362
301.886805	7999.573853	14.260800	-0.061289	4.815234
301.922930	7996.343355	14.265805	-0.061294	4.814290
301.760493	7990.719052	14.270810	-0.061260	4.812648
301.907796	7983.950481	14.275815	-0.061283	4.810669
301.537353	7976.639415	14.280819	-0.061209	4.808533
301.534588	7968.996137	14.285824	-0.061204	4.806297
301.670866	7961.238095	14.290829	-0.061224	4.804025
301.609975	7953.330334	14.295834	-0.061208	4.801710
301.545245	7945.374154	14.300839	-0.061190	4.799380
301.438778	7937.456383	14.305843	-0.061165	4.797059
301.623864	7929.383986	14.310848	-0.061195	4.794691
301.582363	7921.378143	14.315853	-0.061182	4.792343
301.411565	7913.352045	14.320858	-0.061145	4.789987
301.766293	7905.419323	14.325863	-0.061205	4.787656
301.409274	7897.386811	14.330867	-0.061134	4.785297
301.533246	7889.409694	14.335872	-0.061152	4.782952
301.535406	7881.414616	14.340877	-0.061147	4.780600
301.255853	7873.375118	14.345882	-0.061090	4.778236
301.297597	7865.433055	14.350887	-0.061092	4.775897
301.362216	7857.399807	14.355891	-0.061099	4.773531
301.318988	7849.310878	14.360896	-0.061086	4.771147
301.363261	7841.364750	14.365901	-0.061089	4.768804
301.284062	7833.365948	14.370906	-0.061069	4.766445
301.203656	7825.390166	14.375911	-0.061049	4.764091
301.102064	7817.396967	14.380915	-0.061024	4.761731
301.089878	7809.361307	14.385920	-0.061017	4.759357
301.185855	7801.433373	14.390925	-0.061030	4.757014
301.104413	7793.326781	14.395930	-0.061009	4.754617
300.987491	7785.319909	14.400935	-0.060982	4.752248
300.974220	7777.309809	14.405939	-0.060974	4.749877
300.826563	7769.326481	14.410944	-0.060942	4.747513
301.007284	7761.295975	14.415949	-0.060970	4.745133
300.797501	7753.345300	14.420954	-0.060926	4.742776
300.890576	7745.348159	14.425959	-0.060938	4.740404
300.711133	7737.359567	14.430963	-0.060899	4.738033
300.643396	7729.319407	14.435968	-0.060882	4.735646
300.696792	7721.311846	14.440973	-0.060886	4.733267
300.622546	7713.245109	14.445978	-0.060867	4.730870
300.704554	7705.303631	14.450983	-0.060877	4.728508
300.581777	7697.292863	14.455987	-0.060849	4.726125
300.629768	7689.302419	14.460992	-0.060853	4.723747
300.602947	7681.323711	14.465997	-0.060843	4.721370
300.319085	7673.288146	14.471002	-0.060785	4.718977
300.698140	7665.358726	14.476007	-0.060850	4.716612
300.778572	7657.306143	14.481011	-0.060860	4.714210
300.540467	7649.281207	14.486016	-0.060810	4.711816
300.570303	7641.305430	14.491021	-0.060811	4.709434
300.433046	7633.262391	14.496026	-0.060780	4.707032
300.674364	7625.269184	14.501031	-0.060820	4.704642
300.436623	7617.334893	14.506035	-0.060770	4.702270
300.477093	7609.270028	14.511040	-0.060772	4.699857
300.641359	7601.374904	14.516045	-0.060798	4.697493
300.179232	7593.282500	14.521050	-0.060706	4.695071
300.437155	7585.260636	14.526055	-0.060749	4.692666
300.505735	7577.256164	14.531059	-0.060757	4.690267
300.322884	7569.297923	14.536064	-0.060718	4.687880
300.258685	7561.280041	14.541069	-0.060700	4.685474
300.132103	7553.278425	14.546074	-0.060672	4.683071
300.225524	7545.294668	14.551079	-0.060684	4.680673
300.123554	7537.297308	14.556083	-0.060660	4.678269
300.147579	7529.252867	14.561088	-0.060659	4.675850
300.179746	7521.194995	14.566093	-0.060660	4.673425
299.931520	7513.127511	14.571098	-0.060608	4.670997
300.112036	7505.185475	14.576103	-0.060637	4.668604
300.063518	7497.200864	14.581107	-0.060622	4.666198
299.980847	7489.235781	14.586112	-0.060602	4.663797
299.993373	7481.243152	14.591117	-0.060599	4.661386
299.838480	7473.224029	14.596122	-0.060565	4.658966
299.902746	7465.261620	14.601127	-0.060572	4.656561
299.752653	7457.233353	14.606131	-0.060538	4.654136
299.831024	7449.200790	14.611136	-0.060548	4.651707
299.908621	7441.202325	14.616141	-0.060557	4.649288
299.773316	7433.222860	14.621146	-0.060527	4.646873
299.621963	7425.187770	14.626151	-0.060493	4.644441
299.662134	7417.223374	14.631155	-0.060495	4.642028
299.713522	7409.182814	14.636160	-0.060500	4.639591
299.823276	7401.278334	14.641165	-0.060515	4.637194
299.776875	7393.190383	14.646170	-0.060501	4.634740
299.733412	7385.191056	14.651175	-0.060488	4.632312
299.603752	7377.155741	14.656179	-0.060458	4.629871
299.500624	7369.182274	14.661184	-0.060434	4.627448
299.783367	7361.172406	14.666189	-0.060481	4.625013
299.489926	7353.193818	14.671194	-0.060422	4.622586
299.375619	7345.180707	14.676199	-0.060395	4.620147
299.454164	7337.218109	14.681203	-0.060405	4.617722
299.515641	7329.146983	14.686208	-0.060411	4.615263
299.465337	7321.171246	14.691213	-0.060396	4.612831
299.284955	7313.106628	14.696218	-0.060357	4.610372
299.263461	7305.162949	14.701223	-0.060348	4.607947
299.270936	7297.131456	14.706227	-0.060344	4.605495
299.050010	7289.205531	14.711232	-0.060298	4.603074
299.248657	7281.195716	14.716237	-0.060330	4.600625
299.166632	7273.165883	14.721242	-0.060309	4.598170
299.059574	7265.169991	14.726247	-0.060284	4.595723
299.145164	7257.133283	14.731251	-0.060295	4.593262
298.901428	7249.100359	14.736256	-0.060244	4.590802
298.904984	7241.140655	14.741261	-0.060240	4.588362
298.804662	7233.098881	14.746266	-0.060216	4.585896
298.779638	7225.161010	14.751271	-0.060206	4.583461
298.769593	7217.134818	14.756275	-0.060199	4.580997
298.843149	7209.115791	14.761280	-0.060207	4.578534
299.021922	7201.125146	14.766285	-0.060235	4.576078
298.976400	7193.107920	14.771290	-0.060222	4.573613
298.817534	7185.086267	14.776295	-0.060187	4.571145
298.829931	7177.107992	14.781299	-0.060184	4.568689
298.653601	7169.060694	14.786304	-0.060146	4.566211
298.614602	7161.125711	14.791309	-0.060133	4.563766
298.445125	7153.111490	14.796314	-0.060097	4.561295
298.648182	7145.136582	14.801319	-0.060129	4.558835
298.666961	7137.168722	14.806323	-0.060128	4.556376
298.594795	7129.084290	14.811328	-0.060109	4.553879
298.536269	7121.107298	14.816333	-0.060093	4.551414
298.475563	7113.094285	14.821338	-0.060076	4.548937
298.408419	7105.064512	14.826343	-0.060058	4.546453
298.477025	7097.074753	14.831347	-0.060066	4.543980
298.394430	7089.103253	14.836352	-0.060045	4.541512
298.316048	7081.117971	14.841357	-0.060026	4.539038
298.419037	7073.155152	14.846362	-0.060040	4.536569
298.352372	7065.108099	14.851367	-0.060022	4.534073
298.226550	7057.083984	14.856371	-0.059993	4.531583
298.068778	7049.041424	14.861376	-0.059959	4.529085
298.166693	7041.106158	14.866381	-0.059972	4.526620
298.084785	7033.103113	14.871386	-0.059951	4.524132
298.092233	7025.154060	14.876391	-0.059948	4.521660
298.106095	7017.109018	14.881395	-0.059945	4.519156
298.102287	7009.134726	14.886400	-0.059939	4.516673
297.972351	7001.073616	14.891405	-0.059909	4.514162
297.920073	6993.010440	14.896410	-0.059895	4.511648
297.912043	6984.992463	14.901415	-0.059888	4.509148
297.821903	6977.050628	14.906419	-0.059866	4.506669
297.692038	6969.006579	14.911424	-0.059836	4.504157
297.721780	6961.117568	14.916429	-0.059837	4.501693
297.803873	6953.039704	14.921434	-0.059847	4.499168
297.838143	6945.084535	14.926439	-0.059848	4.496680
297.763422	6937.063944	14.931443	-0.059829	4.494170
297.789214	6929.045938	14.936448	-0.059828	4.491659
297.795562	6921.044553	14.941453	-0.059824	4.489153
297.536862	6913.050218	14.946458	-0.059771	4.486646
297.719764	6905.010307	14.951463	-0.059800	4.484125
297.761267	6897.069775	14.956467	-0.059802	4.481633
297.405058	6889.060211	14.961472	-0.059731	4.479117
297.362933	6881.097700	14.966477	-0.059718	4.476616
297.393306	6873.028677	14.971482	-0.059718	4.474079
297.434134	6864.988920	14.976487	-0.059721	4.471551
297.548678	6856.980657	14.981491	-0.059737	4.469031
297.494709	6848.996615	14.986496	-0.059721	4.466517
297.546325	6841.040654	14.991501	-0.059726	4.464011
297.242236	6833.013097	14.996506	-0.059664	4.461479
297.495588	6825.032106	15.001511	-0.059706	4.458963
297.342376	6817.041634	15.006515	-0.059672	4.456440
297.204377	6808.978472	15.011520	-0.059641	4.453894
297.167429	6800.996768	15.016525	-0.059629	4.451372
297.062502	6792.990851	15.021530	-0.059604	4.448840
297.085099	6784.980010	15.026535	-0.059603	4.446307
297.025413	6777.034962	15.031539	-0.059587	4.443792
297.211529	6768.997565	15.036544	-0.059617	4.441247
297.097922	6761.023887	15.041549	-0.059590	4.438720
297.008911	6753.028872	15.046554	-0.059568	4.436185
296.920708	6744.990248	15.051559	-0.059547	4.433635
296.927042	6736.962837	15.056563	-0.059543	4.431087
296.984011	6728.952108	15.061568	-0.059548	4.428543
297.045325	6720.935100	15.066573	-0.059554	4.425996
296.903227	6712.958048	15.071578	-0.059523	4.423459
296.841806	6704.947165	15.076583	-0.059506	4.420910
296.882684	6696.990391	15.081587	-0.059508	4.418378
296.952044	6688.942686	15.086592	-0.059516	4.415815
296.919806	6680.969747	15.091597	-0.059505	4.413274
296.714187	6672.929725	15.096602	-0.059461	4.410709
296.871543	6664.972890	15.101607	-0.059485	4.408171
296.914321	6656.982322	15.106611	-0.059488	4.405621
296.683669	6648.968534	15.111616	-0.059440	4.403060
296.491146	6640.996971	15.116621	-0.059399	4.400511
296.503537	6633.005258	15.121626	-0.059396	4.397955
296.638910	6624.959569	15.126631	-0.059416	4.395381
296.606725	6616.986689	15.131635	-0.059405	4.392829
296.329332	6608.898924	15.136640	-0.059348	4.390236
296.460208	6600.985236	15.141645	-0.059367	4.387700
296.403807	6592.932412	15.146650	-0.059351	4.385117
296.427984	6584.956853	15.151655	-0.059351	4.382558
296.369827	6576.986449	15.156659	-0.059335	4.379998
296.287230	6568.993006	15.161664	-0.059314	4.377429
296.355292	6560.979219	15.166669	-0.059322	4.374853
296.180669	6552.953263	15.171674	-0.059284	4.372270
296.092107	6544.919857	15.176679	-0.059262	4.369684
296.080928	6536.985733	15.181683	-0.059255	4.367129
296.083555	6528.932033	15.186688	-0.059250	4.364533
296.155769	6520.996979	15.191693	-0.059258	4.361975
296.047213	6512.972362	15.196698	-0.059233	4.359385
296.213611	6505.007117	15.201703	-0.059259	4.356815
296.182627	6496.960563	15.206707	-0.059248	4.354216
296.091109	6488.865967	15.211712	-0.059225	4.351599
296.064432	6480.906226	15.216717	-0.059215	4.349024
295.910982	6472.916184	15.221722	-0.059181	4.346438
295.839685	6464.912891	15.226727	-0.059163	4.343846
295.766001	6456.962628	15.231731	-0.059144	4.341270
295.931159	6448.969755	15.236736	-0.059170	4.338680
295.999501	6440.980759	15.241741	-0.059177	4.336089
295.749818	6432.887912	15.246746	-0.059125	4.333460
295.797597	6424.883053	15.251751	-0.059129	4.330861
295.766017	6416.976915	15.256755	-0.059118	4.328291
295.785269	6408.911200	15.261760	-0.059116	4.325669
295.747892	6400.969621	15.266765	-0.059104	4.323085
295.434070	6392.938317	15.271770	-0.059040	4.320468
295.494556	6384.933290	15.276775	-0.059046	4.317861
295.408134	6376.954610	15.281779	-0.059025	4.315260
295.327964	6368.904084	15.286784	-0.059005	4.312633
295.309535	6360.878117	15.291789	-0.058996	4.310014
295.272563	6352.895708	15.296794	-0.058984	4.307407
295.107306	6344.918299	15.301799	-0.058948	4.304799
295.289535	6336.943303	15.306803	-0.058977	4.302193
295.100166	6328.878903	15.311808	-0.058936	4.299554
295.203189	6320.973641	15.316813	-0.058951	4.296967
295.036468	6312.883352	15.321818	-0.058914	4.294316
295.085853	6304.898557	15.326823	-0.058918	4.291699
294.940534	6296.891059	15.331827	-0.058886	4.289072
294.818423	6288.906979	15.336832	-0.058858	4.286451
294.864382	6280.913178	15.341837	-0.058861	4.283827
294.886122	6272.915376	15.346842	-0.058860	4.281199
294.787013	6264.923655	15.351847	-0.058836	4.278571
294.806053	6256.918687	15.356851	-0.058835	4.275938
294.767951	6248.869869	15.361856	-0.058822	4.273288
294.576921	6240.830990	15.366861	-0.058782	4.270639
294.764397	6232.876292	15.371866	-0.058811	4.268019
294.691350	6224.841479	15.376871	-0.058793	4.265369
294.393993	6216.918863	15.381875	-0.058732	4.262752
294.478431	6208.836944	15.386880	-0.058742	4.260084
294.594216	6200.908472	15.391885	-0.058759	4.257466
294.630209	6192.880325	15.396890	-0.058760	4.254812
294.535908	6184.839986	15.401895	-0.058738	4.252151
294.407091	6176.848106	15.406899	-0.058708	4.249505
294.322565	6168.859094	15.411904	-0.058687	4.246858
294.345737	6160.886223	15.416909	-0.058686	4.244216
294.426651	6152.935513	15.421914	-0.058696	4.241580
294.428296	6144.885684	15.426919	-0.058691	4.238909
294.309049	6136.928978	15.431923	-0.058664	4.236266
294.067817	6128.906586	15.436928	-0.058614	4.233598
294.204330	6120.856850	15.441933	-0.058634	4.230923
294.122341	6112.899195	15.446938	-0.058614	4.228275
294.155590	6104.846622	15.451943	-0.058615	4.225595
294.230909	6096.915034	15.456947	-0.058623	4.222954
294.154452	6088.844003	15.461952	-0.058604	4.220263
294.161145	6080.945989	15.466957	-0.058600	4.217629
294.170903	6072.928440	15.471962	-0.058597	4.214953
294.108547	6064.930316	15.476967	-0.058580	4.212282
294.138761	6056.884044	15.481971	-0.058580	4.209593
294.180339	6048.914434	15.486976	-0.058583	4.206929
294.273204	6040.924960	15.491981	-0.058595	4.204257
294.057185	6032.937068	15.496986	-0.058549	4.201580
293.998404	6024.942931	15.501991	-0.058533	4.198902
293.999299	6016.950191	15.506995	-0.058528	4.196222
293.931106	6008.830763	15.512000	-0.058510	4.193498
293.883363	6000.826647	15.517005	-0.058496	4.190811
293.694364	5992.806193	15.522010	-0.058456	4.188115
293.867250	5984.835985	15.527015	-0.058483	4.185438
293.885764	5976.884165	15.532019	-0.058481	4.182764
293.641645	5968.885702	15.537024	-0.058430	4.180070
293.734694	5960.903698	15.542029	-0.058442	4.177383
293.863196	5952.889508	15.547034	-0.058461	4.174684
293.608037	5944.886695	15.552039	-0.058408	4.171983
293.696116	5936.857381	15.557043	-0.058419	4.169275
293.571565	5928.881987	15.562048	-0.058391	4.166581
293.622637	5920.864312	15.567053	-0.058395	4.163873
293.538955	5912.881339	15.572058	-0.058375	4.161173
293.586594	5904.909256	15.577063	-0.058378	4.158477
293.653979	5896.916759	15.582067	-0.058386	4.155773
293.194255	5888.863786	15.587072	-0.058295	4.153040
293.305511	5880.844377	15.592077	-0.058310	4.150323
293.479652	5872.867556	15.597082	-0.058337	4.147620
293.336465	5864.827001	15.602087	-0.058306	4.144889
293.216740	5856.887478	15.607091	-0.058278	4.142191
293.197299	5848.858704	15.612096	-0.058269	4.139463
293.256023	5840.893026	15.617101	-0.058275	4.136755
293.084032	5832.871116	15.622106	-0.058238	4.134023
292.883738	5824.829027	15.627111	-0.058195	4.131282
293.242654	5816.852695	15.632115	-0.058257	4.128569
293.022171	5808.830272	15.637120	-0.058211	4.125831
292.979121	5800.892758	15.642125	-0.058197	4.123122
293.014458	5792.879894	15.647130	-0.058199	4.120387
292.959041	5784.890321	15.652135	-0.058183	4.117657
293.015117	5776.872714	15.657139	-0.058188	4.114917
292.912729	5768.822568	15.662144	-0.058164	4.112161
293.114532	5760.816572	15.667149	-0.058196	4.109423
292.864494	5752.840206	15.672154	-0.058145	4.106688
292.671867	5744.830663	15.677159	-0.058104	4.103940
292.807611	5736.895921	15.682163	-0.058124	4.101220
292.657996	5728.888238	15.687168	-0.058091	4.098470
292.654799	5720.866722	15.692173	-0.058085	4.095714
292.735929	5712.869136	15.697178	-0.058095	4.092967
292.733395	5704.852931	15.702183	-0.058089	4.090210
292.471875	5696.878578	15.707187	-0.058035	4.087462
292.399361	5688.856050	15.712192	-0.058016	4.084698
292.644203	5680.918810	15.717197	-0.058057	4.081966
292.717044	5672.909461	15.722202	-0.058065	4.079205
292.512927	5664.971738	15.727207	-0.058022	4.076463
292.538241	5656.918175	15.732211	-0.058021	4.073682
292.428777	5648.853868	15.737216	-0.057996	4.070894
292.513017	5640.888373	15.742221	-0.058006	4.068140
292.530147	5632.867841	15.747226	-0.058004	4.065365
292.435424	5624.910538	15.752231	-0.057981	4.062608
292.298703	5616.909069	15.757235	-0.057951	4.059834
292.267173	5608.906090	15.762240	-0.057940	4.057058
292.325140	5600.902198	15.767245	-0.057945	4.054282
292.092393	5592.903304	15.772250	-0.057897	4.051501
292.091178	5584.876959	15.777255	-0.057891	4.048712
292.207901	5576.905046	15.782259	-0.057908	4.045942
292.115924	5568.926740	15.787264	-0.057885	4.043165
292.059645	5560.936312	15.792269	-0.057870	4.040382
292.082180	5552.950746	15.797274	-0.057869	4.037600
292.143525	5544.909943	15.802279	-0.057875	4.034797
292.152369	5536.808986	15.807283	-0.057871	4.031971
291.867595	5528.831880	15.812288	-0.057813	4.029181
292.073844	5520.873049	15.817293	-0.057846	4.026404
291.963351	5512.862926	15.822298	-0.057820	4.023602
291.951013	5504.878222	15.827303	-0.057813	4.020808
292.079625	5496.915164	15.832307	-0.057832	4.018022
291.749396	5488.893236	15.837312	-0.057765	4.015206
291.864183	5480.883144	15.842317	-0.057781	4.012399
292.006533	5472.849812	15.847322	-0.057802	4.009583
291.730856	5464.893231	15.852327	-0.057746	4.006785
291.662441	5456.904587	15.857331	-0.057728	4.003977
291.488437	5448.911261	15.862336	-0.057690	4.001164
291.725469	5440.907657	15.867341	-0.057729	3.998351
291.793282	5432.882730	15.872346	-0.057737	3.995527
291.542443	5424.865631	15.877351	-0.057685	3.992698
291.576813	5416.881941	15.882355	-0.057686	3.989884
291.406985	5408.870841	15.887360	-0.057649	3.987054
291.351291	5400.877897	15.892365	-0.057633	3.984231
291.456680	5392.910536	15.897370	-0.057648	3.981417
291.507584	5384.903655	15.902375	-0.057652	3.978587
291.497570	5376.891202	15.907379	-0.057645	3.975751
291.439829	5368.877030	15.912384	-0.057629	3.972913
291.481912	5360.860374	15.917389	-0.057632	3.970073
291.375019	5352.929564	15.922394	-0.057607	3.967258
291.227241	5344.891175	15.927399	-0.057574	3.964403
291.245339	5336.960557	15.932403	-0.057572	3.961587
291.103255	5328.934381	15.937408	-0.057540	3.958733
291.033716	5320.982520	15.942413	-0.057522	3.955903
290.993746	5312.920952	15.947418	-0.057510	3.953034
291.130753	5304.887324	15.952423	-0.057530	3.950175
290.953864	5296.909815	15.957427	-0.057492	3.947328
290.825538	5288.905136	15.962432	-0.057463	3.944471
290.901536	5280.959216	15.967437	-0.057472	3.941636
291.041276	5272.938074	15.972442	-0.057492	3.938774
290.850947	5264.938212	15.977447	-0.057452	3.935911
290.649571	5256.988432	15.982451	-0.057409	3.933064
290.838542	5248.921238	15.987456	-0.057439	3.930179
290.761169	5240.962121	15.992461	-0.057419	3.927327
290.885003	5232.934269	15.997466	-0.057437	3.924451
290.952366	5224.948168	16.002471	-0.057445	3.921587
290.920890	5216.997237	16.007475	-0.057433	3.918732
290.721928	5208.979004	16.012480	-0.057391	3.915848
290.773270	5200.973929	16.017485	-0.057396	3.912971
290.831559	5192.900645	16.022490	-0.057401	3.910067
290.577007	5184.941338	16.027495	-0.057349	3.907196
290.641092	5176.941197	16.032499	-0.057355	3.904314
290.613921	5169.002742	16.037504	-0.057345	3.901451
290.524714	5160.973914	16.042509	-0.057323	3.898552
290.340402	5152.976819	16.047514	-0.057284	3.895661
290.456433	5144.955296	16.052519	-0.057300	3.892764
290.428534	5136.970584	16.057523	-0.057290	3.889875
290.272670	5128.966689	16.062528	-0.057255	3.886975
290.365031	5120.978925	16.067533	-0.057267	3.884084
290.454414	5112.996375	16.072538	-0.057279	3.881192
290.374717	5104.967704	16.077543	-0.057259	3.878278
290.221219	5096.976578	16.082547	-0.057225	3.875373
290.020059	5088.755286	16.087552	-0.057182	3.872383
290.145903	5080.767381	16.092557	-0.057200	3.869481
290.187578	5072.844879	16.097562	-0.057203	3.866599
290.065601	5064.904615	16.102567	-0.057175	3.863705
290.199454	5056.926406	16.107571	-0.057195	3.860800
289.923524	5048.967208	16.112576	-0.057138	3.857892
289.960870	5040.949012	16.117581	-0.057140	3.854967
289.937065	5032.947106	16.122586	-0.057130	3.852043
289.766025	5024.930421	16.127591	-0.057093	3.849110
289.775512	5016.960225	16.132595	-0.057090	3.846194
289.833146	5008.961846	16.137600	-0.057095	3.843267
289.825230	5000.993656	16.142605	-0.057089	3.840348
289.685418	4993.021922	16.147610	-0.057057	3.837422
289.611875	4984.993911	16.152615	-0.057038	3.834475
289.736079	4976.972821	16.157619	-0.057056	3.831532
289.637605	4968.972186	16.162624	-0.057033	3.828590
289.622264	4960.969621	16.167629	-0.057025	3.825647
289.598874	4953.028803	16.172634	-0.057015	3.822724
289.514369	4945.034035	16.177639	-0.056994	3.819777
289.559103	4937.060901	16.182643	-0.056997	3.816839
289.692252	4928.999117	16.187648	-0.057017	3.813868
289.537058	4921.013521	16.192653	-0.056983	3.810916
289.432852	4913.078523	16.197658	-0.056958	3.807982
289.380890	4905.014983	16.202663	-0.056943	3.804999
289.585730	4897.084448	16.207667	-0.056976	3.802069
289.353512	4889.054145	16.212672	-0.056928	3.799090
289.528065	4881.056810	16.217677	-0.056955	3.796130
289.502450	4873.055598	16.222682	-0.056945	3.793161
289.232328	4865.008747	16.227687	-0.056890	3.790168
289.330641	4857.049786	16.232691	-0.056903	3.787214
289.363290	4849.033769	16.237696	-0.056904	3.784234
289.244647	4841.099373	16.242701	-0.056876	3.781279
289.004712	4833.095554	16.247706	-0.056826	3.778293
288.992745	4825.027496	16.252711	-0.056819	3.775286
289.182284	4817.059961	16.257715	-0.056849	3.772319
288.985109	4809.017562	16.262720	-0.056807	3.769312
289.089849	4801.063552	16.267725	-0.056821	3.766343
288.956878	4793.061000	16.272730	-0.056791	3.763348
288.761041	4785.100424	16.277735	-0.056750	3.760365
288.828360	4777.111762	16.282739	-0.056757	3.757375
288.911091	4769.053541	16.287744	-0.056767	3.754357
288.731599	4761.093693	16.292749	-0.056729	3.751368
288.697488	4753.057268	16.297754	-0.056717	3.748350
288.654174	4745.045353	16.302759	-0.056704	3.745339
288.884441	4737.095884	16.307763	-0.056741	3.742356
288.658340	4729.076715	16.312768	-0.056694	3.739333
288.603013	4721.151203	16.317773	-0.056679	3.736347
288.943903	4713.077937	16.322778	-0.056737	3.733313
288.826839	4705.051597	16.327783	-0.056710	3.730282
288.538525	4697.150154	16.332787	-0.056651	3.727293
288.517389	4689.104390	16.337792	-0.056642	3.724253
288.634988	4681.136429	16.342797	-0.056659	3.721243
288.584971	4673.153422	16.347802	-0.056644	3.718221
288.379559	4665.136632	16.352807	-0.056601	3.715179
288.535706	4657.061260	16.357811	-0.056624	3.712122
288.484070	4649.076630	16.362816	-0.056610	3.709092
288.360906	4641.108936	16.367821	-0.056581	3.706064
288.215220	4633.123814	16.372826	-0.056549	3.703026
288.090265	4625.136581	16.377831	-0.056521	3.699986
288.211241	4617.176817	16.382835	-0.056538	3.696959
288.235260	4609.126644	16.387840	-0.056537	3.693894
288.094709	4601.141435	16.392845	-0.056506	3.690846
287.917044	4593.161244	16.397850	-0.056467	3.687797
288.056774	4585.143073	16.402855	-0.056488	3.684738
288.052081	4577.212112	16.407859	-0.056482	3.681707
287.924006	4569.195535	16.412864	-0.056453	3.678638
287.877123	4561.215354	16.417869	-0.056439	3.675582
287.977680	4553.183928	16.422874	-0.056453	3.672507
287.734540	4545.160251	16.427879	-0.056402	3.669424
287.826419	4537.198162	16.432883	-0.056414	3.666371
287.621505	4529.188743	16.437888	-0.056371	3.663289
287.813663	4521.213707	16.442893	-0.056401	3.660228
287.576499	4513.249224	16.447898	-0.056352	3.657158
287.482717	4505.210477	16.452903	-0.056329	3.654060
287.716997	4497.184567	16.457907	-0.056368	3.650973
287.660621	4489.177131	16.462912	-0.056352	3.647883
287.611503	4481.184096	16.467917	-0.056338	3.644795
287.422112	4473.268082	16.472922	-0.056297	3.641732
287.422466	4465.235179	16.477927	-0.056292	3.638625
287.544771	4457.262792	16.482931	-0.056310	3.635543
287.567856	4449.179936	16.487936	-0.056309	3.632413
287.479868	4441.192257	16.492941	-0.056287	3.629313
287.434475	4433.227778	16.497946	-0.056273	3.626222
287.211513	4425.232714	16.502951	-0.056227	3.623111
287.353110	4417.242344	16.507955	-0.056248	3.620009
287.185214	4409.262878	16.512960	-0.056211	3.616900
287.121562	4401.275791	16.517965	-0.056194	3.613788
287.359667	4393.235048	16.522970	-0.056233	3.610661
287.348522	4385.276443	16.527975	-0.056226	3.607557
287.186323	4377.278682	16.532979	-0.056191	3.604430
286.977845	4369.314399	16.537984	-0.056147	3.601312
287.061229	4361.346627	16.542989	-0.056157	3.598199
286.960140	4353.351898	16.547994	-0.056133	3.595067
286.943698	4345.282429	16.552999	-0.056125	3.591905
287.082586	4337.309966	16.558003	-0.056145	3.588783
286.995641	4329.301057	16.563008	-0.056124	3.585638
287.025102	4321.335282	16.568013	-0.056124	3.582510
287.110473	4313.346199	16.573018	-0.056135	3.579371
286.987792	4305.375275	16.578023	-0.056107	3.576232
287.020194	4297.385034	16.583027	-0.056108	3.573086
286.716474	4289.326672	16.588032	-0.056046	3.569901
286.816898	4281.370957	16.593037	-0.056059	3.566765
286.858241	4273.393354	16.598042	-0.056062	3.563616
286.774677	4265.391736	16.603047	-0.056041	3.560451
286.849350	4257.420282	16.608051	-0.056050	3.557300
286.661881	4249.374417	16.613056	-0.056010	3.554109
286.567981	4241.294261	16.618061	-0.055987	3.550905
286.582052	4233.339281	16.623066	-0.055984	3.547750
286.471196	4225.320536	16.628071	-0.055958	3.544563
286.602725	4217.414978	16.633075	-0.055978	3.541426
286.239439	4209.413883	16.638080	-0.055905	3.538233
286.426297	4201.374031	16.643085	-0.055934	3.535038
286.320934	4193.402602	16.648090	-0.055910	3.531859
286.068622	4185.394753	16.653095	-0.055857	3.528658
286.234869	4177.382842	16.658099	-0.055883	3.525465
286.165371	4169.434337	16.663104	-0.055865	3.522288
286.183006	4161.411473	16.668109	-0.055863	3.519080
286.107908	4153.453696	16.673114	-0.055844	3.515893
286.042010	4145.426908	16.678119	-0.055826	3.512675
286.046329	4137.436354	16.683123	-0.055822	3.509472
285.862980	4129.455902	16.688128	-0.055783	3.506263
285.966966	4121.455204	16.693133	-0.055797	3.503052
286.049923	4113.467308	16.698138	-0.055807	3.499843
285.796176	4105.495019	16.703143	-0.055755	3.496627
286.080224	4097.486769	16.708147	-0.055802	3.493410
285.992714	4089.482262	16.713152	-0.055781	3.490180
285.817963	4081.515234	16.718157	-0.055743	3.486959
285.707884	4073.536673	16.723162	-0.055717	3.483733
285.880768	4065.529419	16.728167	-0.055744	3.480501
285.849945	4057.571802	16.733171	-0.055733	3.477280
285.838345	4049.540708	16.738176	-0.055726	3.474027
285.678488	4041.532739	16.743181	-0.055691	3.470775
285.924627	4033.531646	16.748186	-0.055732	3.467536
285.695246	4025.514309	16.753191	-0.055684	3.464272
285.731713	4017.620045	16.758195	-0.055685	3.461063
285.638231	4009.577856	16.763200	-0.055663	3.457787
285.531360	4001.565859	16.768205	-0.055638	3.454520
285.437012	3993.598757	16.773210	-0.055615	3.451268
285.620074	3985.557990	16.778215	-0.055644	3.447993
285.655982	3977.584027	16.783219	-0.055645	3.444737
285.517126	3969.608844	16.788224	-0.055614	3.441471
285.345346	3961.646258	16.793229	-0.055577	3.438206
285.280039	3953.645337	16.798234	-0.055560	3.434926
285.253068	3945.620052	16.803239	-0.055549	3.431634
285.338224	3937.610047	16.808243	-0.055560	3.428350
285.275941	3929.606090	16.813248	-0.055543	3.425059
285.180693	3921.656575	16.818253	-0.055520	3.421786
285.159573	3913.710888	16.823258	-0.055511	3.418515
285.291185	3905.654197	16.828263	-0.055530	3.415200
285.459223	3897.654466	16.833267	-0.055556	3.411906
285.173552	3889.686382	16.838272	-0.055498	3.408607
285.192780	3881.665333	16.843277	-0.055496	3.405293
285.080633	3873.738465	16.848282	-0.055470	3.402010
284.848168	3865.748706	16.853287	-0.055422	3.398694
284.883783	3857.798643	16.858291	-0.055423	3.395400
284.886499	3849.689802	16.863296	-0.055419	3.392036
284.853141	3841.662674	16.868301	-0.055407	3.388701
284.847431	3833.700442	16.873306	-0.055401	3.385391
284.907325	3825.684970	16.878311	-0.055407	3.382058
285.009915	3817.738946	16.883315	-0.055421	3.378752
284.802863	3809.764042	16.888320	-0.055377	3.375420
284.659631	3801.758791	16.893325	-0.055345	3.372074
284.684983	3793.792013	16.898330	-0.055345	3.368747
284.612620	3785.786220	16.903335	-0.055326	3.365397
284.513869	3777.842136	16.908339	-0.055302	3.362068
284.550472	3769.819139	16.913344	-0.055304	3.358708
284.519876	3761.818863	16.918349	-0.055293	3.355352
284.531842	3753.814026	16.923354	-0.055290	3.351992
284.457170	3745.794252	16.928359	-0.055271	3.348619
284.616276	3737.823932	16.933363	-0.055295	3.345271
284.335508	3729.877443	16.938368	-0.055238	3.341915
284.183125	3721.882017	16.943373	-0.055204	3.338539
284.230099	3713.875165	16.948378	-0.055208	3.335162
284.041422	3705.874820	16.953383	-0.055167	3.331776
284.101868	3697.888944	16.958387	-0.055173	3.328402
284.107101	3689.891654	16.963392	-0.055169	3.325017
284.082292	3681.922090	16.968397	-0.055159	3.321640
284.102349	3673.925793	16.973402	-0.055158	3.318250
284.056740	3665.918471	16.978407	-0.055144	3.314848
284.038521	3657.907424	16.983411	-0.055136	3.311443
283.877223	3649.921718	16.988416	-0.055100	3.308040
284.019462	3641.920268	16.993421	-0.055122	3.304638
283.949279	3633.987636	16.998426	-0.055103	3.301254
283.809404	3625.981647	17.003431	-0.055072	3.297832
283.886413	3617.993859	17.008435	-0.055081	3.294423
283.700658	3609.996996	17.013440	-0.055041	3.290996
283.765600	3602.006445	17.018445	-0.055048	3.287578
283.861165	3594.009040	17.023450	-0.055061	3.284155
283.766959	3586.053785	17.028455	-0.055038	3.280739
283.783455	3578.072149	17.033459	-0.055036	3.277312
283.639002	3570.064078	17.038464	-0.055004	3.273864
283.522841	3562.041644	17.043469	-0.054977	3.270407
283.481228	3554.075296	17.048474	-0.054964	3.266974
283.419861	3546.064154	17.053479	-0.054947	3.263517
283.413626	3538.094806	17.058483	-0.054941	3.260077
283.359085	3530.131803	17.063488	-0.054926	3.256633
283.618846	3522.086376	17.068493	-0.054969	3.253163
283.522537	3514.095847	17.073498	-0.054946	3.249699
283.192486	3506.142626	17.078503	-0.054879	3.246238
283.404190	3498.152335	17.083507	-0.054913	3.242779
283.292554	3490.154427	17.088512	-0.054887	3.239300
283.303240	3482.208353	17.093517	-0.054884	3.235844
283.329565	3474.158225	17.098522	-0.054884	3.232340
283.224475	3466.093975	17.103527	-0.054859	3.228821
283.097850	3458.127111	17.108531	-0.054830	3.225340
282.988788	3450.172272	17.113536	-0.054805	3.221861
282.989293	3442.185846	17.118541	-0.054800	3.218369
282.931696	3434.212835	17.123546	-0.054784	3.214876
282.805846	3426.219340	17.128551	-0.054755	3.211368
282.992756	3418.224361	17.133555	-0.054785	3.207868
282.971356	3410.231412	17.138560	-0.054775	3.204357
282.794925	3402.295269	17.143565	-0.054737	3.200860
282.935424	3394.319394	17.148570	-0.054758	3.197355
282.962789	3386.278684	17.153575	-0.054758	3.193813
282.970397	3378.276352	17.158579	-0.054754	3.190284
282.719031	3370.297700	17.163584	-0.054702	3.186750
282.919403	3362.318703	17.168589	-0.054735	3.183230
282.705284	3354.357132	17.173594	-0.054689	3.179698
282.365019	3346.418039	17.178599	-0.054621	3.176165
282.543860	3338.378216	17.183603	-0.054649	3.172607
282.846439	3330.307295	17.188608	-0.054700	3.169035
282.661480	3322.375235	17.193613	-0.054660	3.165501
282.569354	3314.454361	17.198618	-0.054638	3.161971
282.691426	3306.413766	17.203623	-0.054656	3.158394
282.591232	3298.440194	17.208627	-0.054632	3.154833
282.369325	3290.428143	17.213632	-0.054585	3.151245
282.234456	3282.436378	17.218637	-0.054555	3.147666
282.211557	3274.452587	17.223642	-0.054545	3.144091
282.184904	3266.463635	17.228647	-0.054535	3.140510
282.284610	3258.488104	17.233651	-0.054549	3.136936
282.178277	3250.494636	17.238656	-0.054524	3.133341
282.032145	3242.494890	17.243661	-0.054491	3.129737
282.190130	3234.522928	17.248666	-0.054515	3.126156
282.010675	3226.560174	17.253671	-0.054477	3.122559
281.963566	3218.584581	17.258675	-0.054463	3.118958
281.990050	3210.586053	17.263680	-0.054463	3.115346
282.028322	3202.580441	17.268685	-0.054464	3.111727
282.117397	3194.573548	17.273690	-0.054476	3.108105
281.948277	3186.592099	17.278695	-0.054439	3.104479
281.655094	3178.674412	17.283699	-0.054379	3.100872
281.679256	3170.665603	17.288704	-0.054379	3.097234
281.802391	3162.643219	17.293709	-0.054396	3.093590
281.610216	3154.654430	17.298714	-0.054355	3.089943
281.503444	3146.681614	17.303719	-0.054330	3.086302
281.716064	3138.706494	17.308723	-0.054365	3.082671
281.836000	3130.707043	17.313728	-0.054382	3.079020
281.740360	3122.749795	17.318733	-0.054359	3.075374
281.691361	3114.700593	17.323738	-0.054344	3.071684
281.647379	3106.670102	17.328743	-0.054331	3.067998
281.360215	3098.716893	17.333747	-0.054272	3.064332
281.485217	3090.752261	17.338752	-0.054290	3.060676
281.389907	3082.797957	17.343757	-0.054268	3.057009
281.413966	3074.796325	17.348762	-0.054267	3.053322
281.316705	3066.785716	17.353767	-0.054243	3.049621
281.313376	3058.831936	17.358771	-0.054238	3.045945
281.068946	3050.884979	17.363776	-0.054187	3.042257
280.944062	3042.892317	17.368781	-0.054158	3.038549
281.004141	3034.921274	17.373786	-0.054164	3.034856
281.030343	3026.883455	17.378791	-0.054164	3.031125
280.942109	3018.913724	17.383795	-0.054142	3.027416
281.017319	3010.923382	17.388800	-0.054151	3.023700
280.977776	3002.942076	17.393805	-0.054139	3.019979
281.037601	2994.991003	17.398810	-0.054145	3.016272
280.849924	2986.974745	17.403815	-0.054104	3.012517
280.965745	2978.983433	17.408819	-0.054121	3.008785
280.836641	2971.013729	17.413824	-0.054092	3.005046
280.717775	2963.045616	17.418829	-0.054064	3.001304
280.920421	2955.060901	17.423834	-0.054097	2.997565
280.733921	2947.074735	17.428839	-0.054057	2.993801
280.772405	2939.060972	17.433843	-0.054059	2.990031
280.812516	2931.069041	17.438848	-0.054061	2.986267
280.706356	2923.093454	17.443853	-0.054036	2.982498
280.614511	2915.152235	17.448858	-0.054014	2.978741
280.461865	2907.172168	17.453863	-0.053980	2.974958
280.604874	2899.160208	17.458867	-0.054002	2.971170
280.338675	2891.197583	17.463872	-0.053947	2.967380
280.110464	2883.242512	17.468877	-0.053899	2.963591
280.433726	2875.220788	17.473882	-0.053954	2.959793
280.526766	2867.226101	17.478887	-0.053966	2.955991
280.306998	2859.246574	17.483891	-0.053920	2.952176
280.218068	2851.250933	17.488896	-0.053898	2.948354
280.141953	2843.246695	17.493901	-0.053879	2.944525
280.275046	2835.305859	17.498906	-0.053899	2.940731
280.232967	2827.315441	17.503911	-0.053886	2.936900
280.308364	2819.346754	17.508915	-0.053894	2.933080
280.238530	2811.344491	17.513920	-0.053876	2.929231
280.061464	2803.365135	17.518925	-0.053838	2.925383
279.996509	2795.435927	17.523930	-0.053821	2.921560
279.923487	2787.446222	17.528935	-0.053802	2.917702
279.917190	2779.442363	17.533939	-0.053796	2.913836
279.955124	2771.375891	17.538944	-0.053797	2.909937
279.850212	2763.410669	17.543949	-0.053773	2.906073
279.760896	2755.450515	17.548954	-0.053751	2.902208
279.677685	2747.475281	17.553959	-0.053730	2.898331
279.744557	2739.501851	17.558963	-0.053737	2.894458
279.517548	2731.517821	17.563968	-0.053690	2.890558
279.346835	2723.549953	17.568973	-0.053653	2.886664
279.588969	2715.570634	17.573978	-0.053693	2.882781
279.502154	2707.592016	17.578983	-0.053671	2.878876
279.609283	2699.614087	17.583987	-0.053686	2.874976
279.424766	2691.622903	17.588992	-0.053647	2.871049
279.493363	2683.628376	17.593997	-0.053654	2.867128
279.519375	2675.667299	17.599002	-0.053654	2.863216
279.259414	2667.704237	17.604007	-0.053600	2.859282
279.069213	2659.750115	17.609011	-0.053560	2.855351
279.330378	2651.737801	17.614016	-0.053603	2.851411
279.071703	2643.744038	17.619021	-0.053550	2.847445
279.013170	2635.798776	17.624026	-0.053534	2.843509
278.920367	2627.816818	17.629031	-0.053511	2.839548
278.857161	2619.867202	17.634035	-0.053494	2.835599
279.080905	2611.827629	17.639040	-0.053531	2.831615
279.039097	2603.811961	17.644045	-0.053518	2.827623
278.982500	2595.860023	17.649050	-0.053502	2.823656
278.820007	2587.893898	17.654055	-0.053466	2.819671
279.112683	2579.920690	17.659059	-0.053516	2.815702
279.117364	2571.923672	17.664064	-0.053511	2.811699
278.890503	2563.949713	17.669069	-0.053464	2.807689
278.782531	2556.012737	17.674074	-0.053439	2.803699
278.813429	2548.018356	17.679079	-0.053439	2.799681
278.943518	2540.067351	17.684083	-0.053458	2.795686
278.884810	2532.052331	17.689088	-0.053442	2.791642
278.843347	2524.058082	17.694093	-0.053429	2.787603
278.784951	2516.126150	17.699098	-0.053413	2.783589
278.427240	2508.156703	17.704103	-0.053341	2.779533
278.442554	2500.190706	17.709107	-0.053339	2.775494
278.360302	2492.196075	17.714112	-0.053318	2.771430
278.290085	2484.198317	17.719117	-0.053300	2.767358
278.451386	2476.222016	17.724122	-0.053325	2.763305
278.386548	2468.259377	17.729127	-0.053308	2.759239
278.355177	2460.293586	17.734131	-0.053297	2.755168
278.240987	2452.239564	17.739136	-0.053270	2.751041
278.212129	2444.251568	17.744141	-0.053260	2.746946
278.280959	2436.310174	17.749146	-0.053267	2.742876
278.341862	2428.313475	17.754151	-0.053273	2.738770
278.349479	2420.368380	17.759155	-0.053270	2.734681
278.206408	2412.399770	17.764160	-0.053238	2.730565
277.916193	2404.449856	17.769165	-0.053178	2.726444
277.887024	2396.483479	17.774170	-0.053168	2.722323
277.946491	2388.492707	17.779175	-0.053174	2.718189
277.878189	2380.546752	17.784179	-0.053156	2.714065
277.775190	2372.543783	17.789184	-0.053131	2.709902
277.810575	2364.539593	17.794189	-0.053133	2.705740
277.802327	2356.584067	17.799194	-0.053126	2.701595
277.814170	2348.614423	17.804199	-0.053123	2.697438
277.806456	2340.640905	17.809203	-0.053116	2.693270
277.858060	2332.651124	17.814208	-0.053121	2.689092
277.666368	2324.696553	17.819213	-0.053080	2.684910
277.802004	2316.747585	17.824218	-0.053100	2.680745
277.692576	2308.777683	17.829223	-0.053074	2.676547
277.637546	2300.774653	17.834227	-0.053059	2.672329
277.703936	2292.781957	17.839232	-0.053066	2.668117
277.686193	2284.807355	17.844237	-0.053058	2.663903
277.802714	2276.833142	17.849242	-0.053074	2.659691
277.354725	2268.930395	17.854247	-0.052986	2.655473
277.403275	2260.929803	17.859251	-0.052989	2.651229
277.340985	2252.957910	17.864256	-0.052973	2.646986
277.161948	2244.995285	17.869261	-0.052934	2.642734
277.249691	2237.024795	17.874266	-0.052945	2.638488
277.072230	2229.061174	17.879271	-0.052907	2.634221
277.098961	2221.037013	17.884275	-0.052907	2.629929
276.974698	2213.083850	17.889280	-0.052878	2.625658
277.004835	2205.104568	17.894285	-0.052879	2.621375
277.331782	2197.129980	17.899290	-0.052935	2.617109
277.101393	2189.161156	17.904295	-0.052886	2.612801
276.948366	2181.192530	17.909299	-0.052853	2.608491
277.061047	2173.222581	17.914304	-0.052869	2.604191
276.969426	2165.269855	17.919309	-0.052846	2.599880
277.002832	2157.344686	17.924314	-0.052847	2.595585
276.922414	2149.177481	17.929319	-0.052827	2.591143
276.853054	2141.211850	17.934323	-0.052809	2.586805
276.770074	2133.297959	17.939328	-0.052788	2.582486
276.576717	2125.362352	17.944333	-0.052747	2.578141
276.718115	2117.391585	17.949338	-0.052768	2.573792
276.631132	2109.415978	17.954343	-0.052747	2.569417
276.531219	2101.467002	17.959347	-0.052723	2.565048
276.683981	2093.512762	17.964352	-0.052746	2.560687
276.486545	2085.574917	17.969357	-0.052704	2.556303
276.545428	2077.594010	17.974362	-0.052710	2.551906
276.419510	2069.612156	17.979367	-0.052682	2.547487
276.515431	2061.640266	17.984371	-0.052694	2.543082
276.504167	2053.685640	17.989376	-0.052687	2.538671
276.420211	2045.728550	17.994381	-0.052666	2.534246
276.709809	2037.728746	17.999386	-0.052715	2.529816
276.397328	2029.793440	18.004391	-0.052651	2.525372
276.206193	2021.859267	18.009395	-0.052611	2.520928
276.260442	2013.914698	18.014400	-0.052616	2.516489
276.157640	2005.900169	18.019405	-0.052591	2.511991
276.022831	1997.928899	18.024410	-0.052561	2.507507
276.013432	1989.965239	18.029415	-0.052554	2.503029
276.075759	1981.988029	18.034419	-0.052560	2.498540
276.112998	1974.030562	18.039424	-0.052562	2.494052
276.008442	1966.045871	18.044429	-0.052537	2.489531
276.084207	1958.084321	18.049434	-0.052546	2.485027
275.849383	1950.162338	18.054439	-0.052497	2.480515
275.947956	1942.196213	18.059443	-0.052511	2.475994
276.044452	1934.202391	18.064448	-0.052523	2.471449
275.986650	1926.220630	18.069453	-0.052507	2.466891
275.973880	1918.291974	18.074458	-0.052500	2.462359
275.755549	1910.350866	18.079463	-0.052454	2.457795
275.750067	1902.391060	18.084467	-0.052448	2.453228
275.766854	1894.416018	18.089472	-0.052446	2.448646
275.599837	1886.447253	18.094477	-0.052409	2.444044
275.817757	1878.484872	18.099482	-0.052445	2.439467
275.692537	1870.550641	18.104487	-0.052416	2.434872
275.618422	1862.499230	18.109491	-0.052397	2.430203
275.427194	1854.569107	18.114496	-0.052357	2.425587
275.351171	1846.620979	18.119501	-0.052337	2.420961
275.391037	1838.676482	18.124506	-0.052339	2.416337
275.125701	1830.721906	18.129511	-0.052285	2.411674
275.030126	1822.753654	18.134515	-0.052262	2.407008
274.993228	1814.809872	18.139520	-0.052250	2.402351
274.740997	1806.883629	18.144525	-0.052198	2.397679
274.955448	1798.886855	18.149530	-0.052232	2.392993
274.965650	1790.891871	18.154535	-0.052229	2.388282
274.932687	1782.939023	18.159539	-0.052218	2.383584
274.918639	1775.001441	18.164544	-0.052210	2.378887
274.835081	1767.042826	18.169549	-0.052189	2.374162
274.898119	1759.064905	18.174554	-0.052196	2.369429
274.952782	1751.106624	18.179559	-0.052201	2.364697
274.888791	1743.186495	18.184563	-0.052184	2.359969
274.755038	1735.257499	18.189568	-0.052154	2.355220
274.657311	1727.252975	18.194573	-0.052130	2.350419
274.777257	1719.288418	18.199578	-0.052147	2.345650
274.690300	1711.350375	18.204583	-0.052126	2.340871
274.433597	1703.429371	18.209587	-0.052073	2.336078
274.445386	1695.452640	18.214592	-0.052070	2.331263
274.247107	1687.501113	18.219597	-0.052028	2.326437
274.344358	1679.531068	18.224602	-0.052041	2.321614
274.415017	1671.583451	18.229607	-0.052049	2.316792
274.255228	1663.630796	18.234611	-0.052014	2.311938
274.328619	1655.658928	18.239616	-0.052022	2.307081
274.397492	1647.690120	18.244621	-0.052030	2.302215
274.438702	1639.758444	18.249626	-0.052032	2.297360
274.374314	1631.824482	18.254631	-0.052015	2.292484
274.115210	1623.878219	18.259635	-0.051962	2.287574
274.167266	1615.938915	18.264640	-0.051966	2.282683
274.200789	1607.980268	18.269645	-0.051967	2.277769
274.020955	1600.028213	18.274650	-0.051929	2.272830
273.912321	1592.018617	18.279655	-0.051903	2.267850
273.955702	1584.057753	18.284659	-0.051906	2.262903
274.048096	1576.127966	18.289664	-0.051918	2.257969
273.813016	1568.189311	18.294669	-0.051869	2.252990
273.815706	1560.237500	18.299674	-0.051865	2.248012
273.963773	1552.269850	18.304679	-0.051887	2.243026
273.756730	1544.367382	18.309683	-0.051843	2.238039
273.787109	1536.416071	18.314688	-0.051844	2.233030
273.592737	1528.456256	18.319693	-0.051802	2.227985
273.857380	1520.483014	18.324698	-0.051846	2.222961
273.444560	1512.599825	18.329703	-0.051764	2.217923
273.465835	1504.637285	18.334707	-0.051763	2.212861
273.387189	1496.705283	18.339712	-0.051743	2.207798
273.166104	1488.764975	18.344717	-0.051697	2.202705
273.216997	1480.828653	18.349722	-0.051701	2.197628
273.351684	1472.844121	18.354727	-0.051721	2.192515
273.079835	1464.908968	18.359731	-0.051665	2.187385
272.986796	1456.994592	18.364736	-0.051643	2.182273
272.996705	1449.023418	18.369741	-0.051640	2.177122
272.882787	1441.093975	18.374746	-0.051613	2.171974
272.654852	1433.157364	18.379751	-0.051566	2.166798
272.621381	1425.214794	18.384755	-0.051554	2.161624
272.742944	1417.274626	18.389760	-0.051572	2.156454
272.533556	1409.331072	18.394765	-0.051528	2.151238
272.575175	1401.372203	18.399770	-0.051530	2.146024
272.610660	1393.429240	18.404775	-0.051532	2.140806
272.533938	1385.508678	18.409779	-0.051512	2.135579
272.534182	1377.559432	18.414784	-0.051507	2.130328
272.634544	1369.591355	18.419789	-0.051520	2.125062
272.490697	1361.709574	18.424794	-0.051488	2.119816
272.238097	1353.806377	18.429799	-0.051436	2.114532
272.409932	1345.747316	18.434803	-0.051463	2.109172
272.313414	1337.838760	18.439808	-0.051440	2.103873
272.039888	1329.933723	18.444813	-0.051384	2.098546
271.985321	1322.008159	18.449818	-0.051369	2.093212
272.016061	1314.051339	18.454823	-0.051369	2.087853
271.980660	1306.121290	18.459827	-0.051357	2.082491
271.953003	1298.216986	18.464832	-0.051347	2.077133
271.859431	1290.260280	18.469837	-0.051324	2.071720
272.040009	1282.293116	18.474842	-0.051353	2.066312
272.019568	1274.377845	18.479847	-0.051344	2.060906
271.800883	1266.485697	18.484851	-0.051298	2.055481
271.966527	1258.518707	18.489856	-0.051324	2.050029
271.928848	1250.588313	18.494861	-0.051311	2.044568
271.832803	1242.709601	18.499866	-0.051288	2.039121
271.770645	1234.774683	18.504871	-0.051272	2.033625
271.720282	1226.808051	18.509875	-0.051257	2.028092
271.685964	1218.898226	18.514880	-0.051246	2.022586
271.630787	1210.967213	18.519885	-0.051230	2.017048
271.755144	1203.014745	18.524890	-0.051248	2.011498
271.407063	1195.130700	18.529895	-0.051178	2.005931
271.295974	1187.231003	18.534899	-0.051152	2.000363
271.330651	1179.316925	18.539904	-0.051154	1.994784
271.260853	1171.356714	18.544909	-0.051135	1.989146
271.343084	1163.433838	18.549914	-0.051146	1.983535
271.365544	1155.507353	18.554919	-0.051145	1.977898
271.364620	1147.585054	18.559923	-0.051139	1.972247
271.253013	1139.668635	18.564928	-0.051113	1.966571
270.966130	1131.784836	18.569933	-0.051055	1.960883
271.070419	1123.877452	18.574938	-0.051069	1.955204
270.909054	1115.910736	18.579943	-0.051034	1.949437
270.745784	1107.994470	18.584947	-0.050998	1.943689
270.964718	1100.056724	18.589952	-0.051034	1.937950
270.772369	1092.140181	18.594957	-0.050993	1.932164
270.863279	1084.215248	18.599962	-0.051005	1.926386
270.833166	1076.308840	18.604967	-0.050994	1.920591
270.750953	1068.415283	18.609971	-0.050973	1.914782
270.641717	1060.502644	18.614976	-0.050948	1.908938
270.531637	1052.591864	18.619981	-0.050922	1.903077
270.716135	1044.672185	18.624986	-0.050951	1.897225
270.758597	1036.741749	18.629991	-0.050954	1.891331
270.651298	1028.837219	18.634995	-0.050929	1.885420
270.714228	1020.949733	18.640000	-0.050936	1.879523
270.491299	1013.064893	18.645005	-0.050889	1.873577
270.363063	1005.154170	18.650010	-0.050860	1.867603
270.428487	997.227896	18.655015	-0.050867	1.861621
270.290887	989.342651	18.660019	-0.050836	1.855627
270.291616	981.427148	18.665024	-0.050831	1.849606
270.250201	973.516476	18.670029	-0.050818	1.843565
270.208927	965.640463	18.675034	-0.050805	1.837530
270.194527	957.720858	18.680039	-0.050798	1.831445
270.170042	949.808473	18.685043	-0.050788	1.825344
270.176592	941.936481	18.690048	-0.050784	1.819258
270.032649	934.044514	18.695053	-0.050752	1.813118
269.954934	926.153323	18.700058	-0.050732	1.806965
269.841502	918.264440	18.705063	-0.050706	1.800789
269.801023	910.378060	18.710067	-0.050693	1.794602
269.815889	902.428069	18.715072	-0.050691	1.788351
269.685784	894.542148	18.720077	-0.050662	1.782110
269.584592	886.681593	18.725082	-0.050638	1.775871
269.695847	878.752516	18.730087	-0.050653	1.769582
269.618953	870.873573	18.735091	-0.050634	1.763287
269.595441	863.012513	18.740096	-0.050624	1.756991
269.469082	855.119268	18.745101	-0.050596	1.750633
269.414137	847.241857	18.750106	-0.050580	1.744273
269.384032	839.363488	18.755111	-0.050570	1.737893
269.303016	831.479624	18.760115	-0.050549	1.731478
269.339388	823.589947	18.765120	-0.050551	1.725050
269.231835	815.735463	18.770125	-0.050526	1.718608
269.333912	807.838797	18.775130	-0.050540	1.712134
269.266444	799.946413	18.780135	-0.050522	1.705617
269.037677	792.112663	18.785139	-0.050474	1.699102
269.173338	784.216502	18.790144	-0.050494	1.692559
268.993364	776.349804	18.795149	-0.050456	1.685972
268.869714	768.513419	18.800154	-0.050428	1.679393
268.816727	760.637867	18.805159	-0.050413	1.672765
268.815052	752.742933	18.810163	-0.050407	1.666100
268.883844	744.879728	18.815168	-0.050415	1.659445
268.578239	737.053307	18.820173	-0.050353	1.652744
268.706965	729.154869	18.825178	-0.050372	1.646013
268.798025	721.291825	18.830183	-0.050383	1.639280
268.420709	713.459581	18.835187	-0.050308	1.632481
268.319609	705.572920	18.840192	-0.050284	1.625645
268.341260	697.705026	18.845197	-0.050283	1.618813
268.426936	689.838391	18.850202	-0.050294	1.611962
268.219604	682.003506	18.855207	-0.050250	1.605069
268.067701	674.192818	18.860211	-0.050217	1.598175
268.217522	666.308005	18.865216	-0.050239	1.591228
268.096993	658.463182	18.870221	-0.050212	1.584248
268.229942	650.600777	18.875226	-0.050232	1.577258
268.047068	642.776487	18.880231	-0.050192	1.570225
267.911184	634.954850	18.885235	-0.050162	1.563169
268.006568	627.121709	18.890240	-0.050175	1.556105
267.888152	619.264378	18.895245	-0.050147	1.548956
267.842415	611.436032	18.900250	-0.050134	1.541810
267.776457	603.621219	18.905255	-0.050116	1.534640
268.000407	595.724743	18.910259	-0.050153	1.527405
267.827550	587.942863	18.915264	-0.050116	1.520182
267.693696	580.140111	18.920269	-0.050086	1.512911
267.664823	572.306283	18.925274	-0.050075	1.505592
267.659533	564.493364	18.930279	-0.050069	1.498260
267.486089	556.684490	18.935283	-0.050032	1.490870
267.488014	548.876381	18.940288	-0.050027	1.483471
267.344662	541.085149	18.945293	-0.049995	1.476028
267.493185	533.196926	18.950298	-0.050018	1.468500
267.341517	525.409002	18.955303	-0.049985	1.460983
267.298209	517.612516	18.960307	-0.049971	1.453436
267.037817	509.839835	18.965312	-0.049918	1.445838
267.070482	502.043689	18.970317	-0.049919	1.438224
267.100344	494.232888	18.975322	-0.049919	1.430554
266.898787	486.461855	18.980327	-0.049877	1.422845
266.746136	478.700385	18.985331	-0.049843	1.415111
266.781455	470.887177	18.990336	-0.049845	1.407314
266.816323	463.098265	18.995341	-0.049846	1.399498
266.697928	455.339898	19.000346	-0.049819	1.391643
266.639265	447.551684	19.005351	-0.049803	1.383724
266.530507	439.794393	19.010355	-0.049778	1.375781
266.455572	432.029315	19.015360	-0.049759	1.367791
266.355581	424.267368	19.020365	-0.049735	1.359752
266.389737	416.502140	19.025370	-0.049736	1.351685
266.184915	408.765850	19.030375	-0.049693	1.343559
266.168647	401.013177	19.035379	-0.049685	1.335399
266.098760	393.265586	19.040384	-0.049667	1.327184
265.921264	385.544061	19.045389	-0.049629	1.318927
266.020706	377.704043	19.050394	-0.049642	1.310541
265.983428	369.921147	19.055399	-0.049630	1.302137
265.915276	362.209335	19.060403	-0.049613	1.293750
265.795226	354.504665	19.065408	-0.049585	1.285307
265.802384	346.788107	19.070413	-0.049581	1.276819
265.782150	339.068372	19.075418	-0.049573	1.268265
265.661708	331.378498	19.080423	-0.049545	1.259668
265.578181	323.680567	19.085427	-0.049525	1.251009
265.476047	315.999255	19.090432	-0.049501	1.242305
265.599428	308.288235	19.095437	-0.049519	1.233550
265.624057	300.580294	19.100442	-0.049518	1.224716
265.430964	292.936013	19.105447	-0.049477	1.215849
265.214865	285.277923	19.110451	-0.049432	1.206896
265.382467	277.589861	19.115456	-0.049458	1.197918
265.152176	269.944770	19.120461	-0.049410	1.188842
265.108155	262.299459	19.125466	-0.049397	1.179734
264.982273	254.659397	19.130471	-0.049369	1.170545
265.046008	246.998529	19.135475	-0.049376	1.161297
265.013001	239.365248	19.140480	-0.049364	1.151989
264.628338	231.760571	19.145485	-0.049288	1.142565
264.632139	224.134924	19.150490	-0.049284	1.133120
264.611547	216.510130	19.155495	-0.049275	1.123591
264.410501	208.937666	19.160499	-0.049232	1.114007
264.673183	201.285167	19.165504	-0.049276	1.104340
264.517891	193.724136	19.170509	-0.049243	1.094613
264.306893	186.173044	19.175514	-0.049198	1.084799
264.257477	178.617068	19.180519	-0.049184	1.074925
264.278311	171.027977	19.185523	-0.049183	1.064932
264.133955	163.508515	19.190528	-0.049151	1.054900
263.758433	156.016952	19.195533	-0.049077	1.044754
263.863868	148.470516	19.200538	-0.049091	1.034548
263.940910	140.922513	19.205543	-0.049101	1.024231
263.557568	133.479499	19.210547	-0.049024	1.013843
263.615531	125.970888	19.215552	-0.049030	1.003364
263.619730	118.471027	19.220557	-0.049026	0.992773
263.500505	110.994757	19.225562	-0.048999	0.982071
263.403775	103.551014	19.230567	-0.048976	0.971304
263.361251	96.107023	19.235571	-0.048964	0.960430
263.572480	88.649078	19.240576	-0.048998	0.949476
263.189048	81.299003	19.245581	-0.048922	0.938400
263.186481	73.898549	19.250586	-0.048917	0.927217
263.204782	66.523884	19.255591	-0.048915	0.915942
262.918799	59.423507	19.260595	-0.048857	0.904871