Fri Mar 12 12:01:09 2021


Number of Points = 3624

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.946618	-0.017950	0.000000	0.000007	0.721072
0.802034	0.006835	0.005005	0.000034	0.721070
0.820859	-0.061865	0.010010	0.000031	0.720942
0.781634	-0.093841	0.015014	0.000038	0.720865
1.027554	-0.132408	0.020019	-0.000008	0.720875
0.977101	-0.126368	0.025024	0.000002	0.720870
1.005245	-0.129247	0.030029	-0.000003	0.720874
0.922921	-0.112970	0.035034	0.000012	0.720877
0.960400	-0.123184	0.040038	0.000005	0.720870
1.000785	-0.127093	0.045043	-0.000003	0.720877
0.830431	-0.100217	0.050048	0.000029	0.720870
0.944863	-0.118343	0.055053	0.000008	0.720874
0.950555	-0.119485	0.060058	0.000007	0.720874
0.864132	-0.106127	0.065062	0.000023	0.720870
1.155732	-0.151837	0.070067	-0.000032	0.720882
0.943165	-0.121013	0.075072	0.000008	0.720869
0.829458	-0.225892	0.080077	0.000029	0.720622
1.011066	-0.301221	0.085082	-0.000005	0.720538
0.954365	-0.294622	0.090086	0.000006	0.720531
1.129375	-0.319573	0.095091	-0.000027	0.720543
1.032141	-0.306787	0.100096	-0.000008	0.720534
1.146478	-0.325056	0.105101	-0.000030	0.720538
1.107060	-0.400223	0.110106	-0.000022	0.720377
0.822561	-0.429744	0.115110	0.000031	0.720219
1.013078	-0.459640	0.120115	-0.000005	0.720227
0.952422	-0.454157	0.125120	0.000006	0.720216
1.048694	-0.468894	0.130125	-0.000012	0.720221
1.091948	-0.566710	0.135130	-0.000020	0.720043
1.067864	-0.638451	0.140134	-0.000015	0.719894
0.907553	-0.605831	0.145139	0.000015	0.719902
0.920965	-0.611081	0.150144	0.000012	0.719896
0.877468	-0.664180	0.155149	0.000020	0.719776
1.020749	-0.780072	0.160154	-0.000006	0.719598
0.964164	-0.772459	0.165158	0.000004	0.719593
1.169911	-0.804121	0.170163	-0.000034	0.719603
1.097174	-0.920826	0.175168	-0.000020	0.719347
1.004681	-0.945326	0.180173	-0.000003	0.719267
1.033819	-0.947161	0.185178	-0.000009	0.719273
1.018202	-1.019497	0.190182	-0.000006	0.719125
1.018973	-1.100354	0.195187	-0.000006	0.718966
0.802831	-1.065191	0.200192	0.000035	0.718959
0.909118	-1.142079	0.205197	0.000015	0.718845
0.776335	-1.220708	0.210202	0.000040	0.718643
0.659371	-1.201784	0.215206	0.000061	0.718639
0.832675	-1.284731	0.220211	0.000029	0.718537
0.850544	-1.383666	0.225216	0.000026	0.718348
0.774856	-1.368456	0.230221	0.000040	0.718351
0.783611	-1.479374	0.235226	0.000038	0.718135
0.736028	-1.535666	0.240230	0.000047	0.718007
0.926173	-1.571517	0.245235	0.000012	0.718003
0.795711	-1.703240	0.250240	0.000036	0.717697
0.918613	-1.722652	0.255245	0.000013	0.717702
0.982077	-1.829952	0.260250	0.000002	0.717512
0.868837	-1.880295	0.265254	0.000023	0.717373
0.755681	-1.898473	0.270259	0.000044	0.717297
0.808473	-2.019207	0.275264	0.000034	0.717077
0.703999	-1.999028	0.280269	0.000053	0.717080
0.613368	-2.147582	0.285274	0.000070	0.716754
0.540700	-2.138394	0.290278	0.000084	0.716747
0.444611	-2.235715	0.295283	0.000102	0.716520
0.540735	-2.292663	0.300288	0.000084	0.716441
0.494654	-2.378468	0.305293	0.000093	0.716255
0.247198	-2.396383	0.310298	0.000139	0.716132
-0.074563	-2.397544	0.315302	0.000199	0.716017
-0.304011	-2.423805	0.320307	0.000241	0.715884
-2.738609	-1.993585	0.325312	0.000694	0.715877
-2.538328	-2.166191	0.330317	0.000657	0.715605
-2.937907	-2.125530	0.335322	0.000731	0.715545
-3.474035	-2.033457	0.340326	0.000831	0.715538
-2.789881	-2.219978	0.345331	0.000704	0.715410
-4.069674	-2.086881	0.350336	0.000942	0.715222
-3.855471	-2.122139	0.355341	0.000902	0.715228
-3.906107	-2.112576	0.360346	0.000912	0.715229
-4.335951	-2.156279	0.365350	0.000992	0.714990
-4.791740	-2.116114	0.370355	0.001077	0.714909
-5.104354	-2.063892	0.375360	0.001135	0.714902
-5.191196	-2.048942	0.380365	0.001151	0.714901
-4.735149	-2.189148	0.385370	0.001066	0.714784
-6.030203	-2.052094	0.390374	0.001307	0.714598
-5.900346	-2.071504	0.395379	0.001283	0.714605
-5.816971	-2.089826	0.400384	0.001267	0.714598
-5.695442	-2.109088	0.405389	0.001245	0.714603
-5.913330	-2.192601	0.410394	0.001285	0.714360
-7.225387	-2.005186	0.415398	0.001530	0.714268
-6.686995	-2.096871	0.420403	0.001429	0.714277
-6.611543	-2.114921	0.425408	0.001415	0.714268
-7.075483	-2.030821	0.430413	0.001502	0.714270
-6.485633	-2.208997	0.435418	0.001392	0.714125
-7.923451	-2.036706	0.440422	0.001660	0.713959
-7.628587	-2.083083	0.445427	0.001605	0.713971
-7.619928	-2.086049	0.450432	0.001603	0.713968
-7.566266	-2.097740	0.455437	0.001593	0.713964
-7.561754	-2.096865	0.460442	0.001592	0.713967
-8.341207	-2.112756	0.465446	0.001737	0.713660
-8.421289	-2.102580	0.470451	0.001752	0.713651
-8.757925	-2.046263	0.475456	0.001815	0.713644
-8.575360	-2.077897	0.480461	0.001781	0.713646
-8.263971	-2.131815	0.485466	0.001723	0.713649
-8.774159	-2.045558	0.490470	0.001818	0.713640
-8.885798	-2.147118	0.495475	0.001839	0.713398
-9.646302	-2.035252	0.500480	0.001980	0.713351
-9.501096	-2.059249	0.505485	0.001953	0.713355
-9.385376	-2.078621	0.510490	0.001932	0.713358
-9.830743	-2.002379	0.515494	0.002014	0.713352
-9.095163	-2.129719	0.520499	0.001878	0.713359
-9.333509	-2.179153	0.525504	0.001922	0.713176
-10.855342	-1.987052	0.530509	0.002205	0.713019
-10.053954	-2.126868	0.535514	0.002056	0.713025
-10.239680	-2.098139	0.540518	0.002091	0.713016
-10.688754	-2.014566	0.545523	0.002174	0.713023
-10.231958	-2.099220	0.550528	0.002089	0.713017
-10.234665	-2.097884	0.555533	0.002090	0.713018
-10.618730	-2.179217	0.560538	0.002161	0.712720
-11.506828	-2.031219	0.565542	0.002326	0.712700
-11.472963	-2.032519	0.570547	0.002320	0.712709
-11.339175	-2.060561	0.575552	0.002295	0.712701
-11.289090	-2.068279	0.580557	0.002286	0.712704
-11.367013	-2.051621	0.585562	0.002300	0.712709
-11.414410	-2.050634	0.590566	0.002309	0.712694
-11.951268	-2.107215	0.595571	0.002409	0.712391
-12.180366	-2.072516	0.600576	0.002452	0.712379
-12.226906	-2.064703	0.605581	0.002461	0.712378
-12.018870	-2.099077	0.610586	0.002422	0.712383
-12.601561	-2.000472	0.615590	0.002530	0.712373
-12.232676	-2.061352	0.620595	0.002462	0.712383
-12.157473	-2.076681	0.625600	0.002448	0.712379
-13.048652	-2.049648	0.630605	0.002613	0.712116
-13.174577	-2.041320	0.635610	0.002637	0.712088
-13.313449	-2.019522	0.640614	0.002663	0.712082
-13.024600	-2.068220	0.645619	0.002609	0.712088
-13.158738	-2.046873	0.650624	0.002634	0.712083
-13.305808	-2.020324	0.655629	0.002661	0.712084
-12.867187	-2.095866	0.660634	0.002580	0.712089
-13.488997	-2.089443	0.665638	0.002695	0.711881
-14.303146	-2.004674	0.670643	0.002847	0.711761
-13.951930	-2.069576	0.675648	0.002782	0.711756
-14.360705	-1.996863	0.680653	0.002858	0.711756
-14.047327	-2.049503	0.685658	0.002799	0.711762
-14.095348	-2.046985	0.690662	0.002808	0.711750
-14.095091	-2.042812	0.695667	0.002808	0.711759
-14.351000	-2.025837	0.700672	0.002856	0.711702
-14.900040	-2.054584	0.705677	0.002958	0.711449
-14.474850	-2.128755	0.710682	0.002879	0.711452
-15.520355	-1.947157	0.715686	0.003073	0.711443
-14.818236	-2.067115	0.720691	0.002943	0.711453
-14.603564	-2.108274	0.725696	0.002903	0.711447
-15.488171	-1.951003	0.730701	0.003067	0.711447
-15.008098	-2.045168	0.735706	0.002978	0.711430
-15.731631	-2.067331	0.740710	0.003113	0.711128
-15.696868	-2.070641	0.745715	0.003106	0.711134
-15.829896	-2.047453	0.750720	0.003131	0.711133
-15.679889	-2.075406	0.755725	0.003103	0.711131
-15.761895	-2.057008	0.760730	0.003118	0.711138
-16.320343	-1.963409	0.765734	0.003222	0.711126
-15.981043	-2.019188	0.770739	0.003159	0.711136
-16.308901	-2.084190	0.775744	0.003220	0.710889
-16.994944	-1.974614	0.780749	0.003348	0.710864
-16.729486	-2.018722	0.785754	0.003298	0.710870
-16.472527	-2.069292	0.790758	0.003251	0.710861
-16.641025	-2.034740	0.795763	0.003282	0.710870
-16.801425	-2.007495	0.800768	0.003312	0.710867
-16.642384	-2.037839	0.805773	0.003282	0.710863
-16.868429	-2.157867	0.810778	0.003324	0.710543
-17.736064	-2.013224	0.815782	0.003486	0.710523
-17.739078	-2.008476	0.820787	0.003486	0.710532
-17.087631	-2.126296	0.825792	0.003365	0.710528
-17.761785	-2.007769	0.830797	0.003491	0.710525
-17.841050	-1.987635	0.835802	0.003505	0.710537
-17.628207	-2.037728	0.840806	0.003466	0.710513
-18.062128	-2.108556	0.845811	0.003547	0.710217
-18.325317	-2.063616	0.850816	0.003596	0.710213
-18.703334	-1.997001	0.855821	0.003666	0.710212
-18.201655	-2.082313	0.860826	0.003573	0.710220
-18.779066	-1.986258	0.865830	0.003680	0.710206
-18.494248	-2.032845	0.870835	0.003627	0.710214
-18.267852	-2.090894	0.875840	0.003585	0.710179
-19.436306	-2.029808	0.880845	0.003802	0.709885
-19.224029	-2.063940	0.885850	0.003763	0.709892
-19.560884	-2.007977	0.890854	0.003825	0.709884
-19.199378	-2.067414	0.895859	0.003758	0.709894
-19.615082	-1.996814	0.900864	0.003836	0.709887
-19.658361	-1.988877	0.905869	0.003844	0.709888
-18.897080	-2.122683	0.910874	0.003702	0.709892
-20.042449	-2.066308	0.915878	0.003915	0.709596
-20.108993	-2.056215	0.920883	0.003928	0.709593
-19.893898	-2.095611	0.925888	0.003887	0.709591
-20.115433	-2.055944	0.930893	0.003929	0.709591
-20.225977	-2.035199	0.935898	0.003949	0.709593
-20.439953	-2.002264	0.940902	0.003989	0.709583
-19.921318	-2.121239	0.945907	0.003893	0.709530
-21.104736	-2.045518	0.950912	0.004113	0.709259
-21.205526	-2.029124	0.955917	0.004132	0.709256
-21.153759	-2.034576	0.960922	0.004122	0.709264
-21.261223	-2.021167	0.965926	0.004142	0.709252
-21.104054	-2.046184	0.970931	0.004113	0.709258
-20.977238	-2.068678	0.975936	0.004089	0.709258
-21.197667	-2.031391	0.980941	0.004130	0.709254
-21.576519	-2.108088	0.985946	0.004201	0.708966
-22.056536	-2.033735	0.990950	0.004290	0.708943
-21.704447	-2.091739	0.995955	0.004224	0.708953
-21.842321	-2.069009	1.000960	0.004250	0.708949
-22.233013	-2.000946	1.005965	0.004323	0.708946
-21.576001	-2.114426	1.010970	0.004201	0.708953
-21.885151	-2.102415	1.015974	0.004258	0.708867
-23.069547	-2.006465	1.020979	0.004479	0.708637
-22.563671	-2.098897	1.025984	0.004384	0.708632
-22.797809	-2.057760	1.030989	0.004428	0.708631
-22.928901	-2.030002	1.035994	0.004452	0.708640
-22.912295	-2.037530	1.040998	0.004449	0.708631
-22.756782	-2.062880	1.046003	0.004420	0.708635
-22.874093	-2.068050	1.051008	0.004442	0.708583
-23.874057	-2.010216	1.056013	0.004628	0.708342
-23.463523	-2.081371	1.061018	0.004552	0.708346
-23.893149	-2.008702	1.066022	0.004632	0.708338
-23.809938	-2.018751	1.071027	0.004616	0.708348
-23.408144	-2.090802	1.076032	0.004542	0.708347
-23.814814	-2.020744	1.081037	0.004617	0.708342
-23.820335	-2.037025	1.086042	0.004618	0.708307
-24.848612	-2.006445	1.091046	0.004810	0.708001
-24.497126	-2.067078	1.096051	0.004744	0.708005
-24.793339	-2.014486	1.101056	0.004799	0.708005
-24.922204	-1.993357	1.106061	0.004823	0.708001
-24.410527	-2.080712	1.111066	0.004728	0.708009
-24.784943	-2.019242	1.116070	0.004798	0.707999
-24.645093	-2.040947	1.121075	0.004772	0.708005
-24.694455	-2.142786	1.126080	0.004781	0.707783
-25.750050	-2.000062	1.131085	0.004977	0.707692
-25.685028	-2.006952	1.136090	0.004965	0.707702
-25.761076	-2.000333	1.141094	0.004979	0.707688
-25.805094	-1.987633	1.146099	0.004988	0.707698
-25.660876	-2.014048	1.151104	0.004961	0.707696
-25.765871	-1.998612	1.156109	0.004980	0.707690
-25.541936	-2.089665	1.161114	0.004939	0.707587
-26.584753	-2.012530	1.166118	0.005133	0.707369
-26.475837	-2.029502	1.171123	0.005113	0.707374
-26.582165	-2.011959	1.176128	0.005132	0.707371
-26.548054	-2.020733	1.181133	0.005126	0.707366
-26.330722	-2.053841	1.186138	0.005085	0.707377
-26.820235	-1.972431	1.191142	0.005177	0.707365
-26.364796	-2.076490	1.196147	0.005092	0.707319
-27.021943	-2.081894	1.201152	0.005214	0.707073
-27.422286	-2.009960	1.206157	0.005289	0.707075
-27.292386	-2.030402	1.211162	0.005264	0.707080
-27.316190	-2.030679	1.216166	0.005269	0.707071
-27.629859	-1.971861	1.221171	0.005327	0.707077
-27.359841	-2.021089	1.226176	0.005277	0.707075
-27.067660	-2.110424	1.231181	0.005223	0.707000
-27.932001	-2.079767	1.236186	0.005384	0.706752
-28.292806	-2.021486	1.241190	0.005451	0.706740
-28.267909	-2.022319	1.246195	0.005446	0.706747
-28.053739	-2.060349	1.251200	0.005406	0.706747
-28.453614	-1.991101	1.256205	0.005481	0.706743
-28.163475	-2.040535	1.261210	0.005427	0.706748
-27.958397	-2.126838	1.266214	0.005388	0.706648
-28.989132	-2.046294	1.271219	0.005580	0.706441
-28.875505	-2.066559	1.276224	0.005559	0.706441
-29.179360	-2.015006	1.281229	0.005616	0.706436
-28.989883	-2.044402	1.286234	0.005580	0.706444
-29.232456	-2.006415	1.291238	0.005626	0.706434
-29.179899	-2.011210	1.296243	0.005616	0.706443
-28.899447	-2.128014	1.301248	0.005564	0.706309
-30.552434	-1.927717	1.306253	0.005871	0.706119
-29.922897	-2.034862	1.311258	0.005754	0.706129
-29.937106	-2.037697	1.316262	0.005757	0.706119
-30.238304	-1.982190	1.321267	0.005813	0.706122
-30.141721	-1.998911	1.326272	0.005795	0.706123
-30.177271	-1.993632	1.331277	0.005801	0.706121
-29.994644	-2.023401	1.336282	0.005767	0.706127
-30.896168	-1.997045	1.341286	0.005935	0.705857
-31.028862	-1.973012	1.346291	0.005960	0.705857
-30.913625	-1.993098	1.351296	0.005938	0.705858
-31.015058	-1.976423	1.356301	0.005957	0.705856
-30.777232	-2.015064	1.361306	0.005913	0.705863
-30.741890	-2.026418	1.366310	0.005906	0.705853
-30.866367	-2.000784	1.371315	0.005930	0.705860
-31.158242	-2.085186	1.376320	0.005984	0.705586
-32.061116	-1.959697	1.381325	0.006152	0.705514
-31.593745	-2.037322	1.386330	0.006065	0.705526
-31.904335	-1.987199	1.391334	0.006123	0.705515
-31.830985	-1.996173	1.396339	0.006109	0.705523
-31.411493	-2.071158	1.401344	0.006031	0.705523
-31.835423	-1.997961	1.406349	0.006110	0.705518
-32.294658	-2.053852	1.411354	0.006196	0.705241
-32.698875	-2.000838	1.416358	0.006271	0.705203
-32.640184	-2.009333	1.421363	0.006260	0.705207
-32.649200	-2.008239	1.426368	0.006261	0.705206
-32.502657	-2.036389	1.431373	0.006234	0.705202
-32.042625	-2.114649	1.436378	0.006149	0.705209
-32.474060	-2.073568	1.441382	0.006229	0.705137
-33.636948	-1.992389	1.446387	0.006445	0.704883
-33.315076	-2.050051	1.451392	0.006385	0.704883
-33.743029	-1.977332	1.456397	0.006465	0.704875
-33.634114	-1.993038	1.461402	0.006445	0.704883
-33.375734	-2.041397	1.466406	0.006397	0.704878
-33.583077	-2.003163	1.471411	0.006435	0.704881
-33.479603	-2.029641	1.476416	0.006416	0.704865
-34.237728	-2.036216	1.481421	0.006557	0.704579
-34.213512	-2.036940	1.486426	0.006553	0.704586
-34.807761	-1.933331	1.491430	0.006663	0.704582
-34.283226	-2.026622	1.496435	0.006566	0.704582
-33.886237	-2.095896	1.501440	0.006492	0.704585
-34.373343	-2.011621	1.506445	0.006582	0.704580
-34.508288	-2.003957	1.511450	0.006607	0.704547
-35.192356	-2.029239	1.516454	0.006735	0.704250
-34.968999	-2.066785	1.521459	0.006693	0.704255
-35.443153	-1.981680	1.526464	0.006782	0.704256
-35.440319	-1.984092	1.531469	0.006781	0.704252
-34.792715	-2.096616	1.536474	0.006660	0.704258
-35.363562	-2.001009	1.541478	0.006767	0.704246
-35.450078	-1.992756	1.546483	0.006783	0.704231
-35.686585	-2.091492	1.551488	0.006827	0.703947
-36.010745	-2.036997	1.556493	0.006887	0.703941
-36.181923	-2.001225	1.561498	0.006919	0.703951
-36.150823	-2.011268	1.566502	0.006913	0.703942
-35.887287	-2.056637	1.571507	0.006864	0.703945
-36.190579	-2.002148	1.576512	0.006921	0.703946
-36.336514	-2.006786	1.581517	0.006948	0.703885
-36.782150	-2.052188	1.586522	0.007031	0.703633
-37.055169	-2.009323	1.591526	0.007082	0.703621
-37.375512	-1.948621	1.596531	0.007141	0.703628
-36.977395	-2.018257	1.601536	0.007067	0.703631
-37.187663	-1.983640	1.606541	0.007106	0.703625
-37.398356	-1.940940	1.611546	0.007145	0.703636
-37.242804	-1.973673	1.616550	0.007116	0.703625
-36.855766	-2.148655	1.621555	0.007044	0.703412
-38.018100	-1.978894	1.626560	0.007261	0.703336
-38.220449	-1.946150	1.631565	0.007298	0.703329
-37.507920	-2.067091	1.636570	0.007166	0.703342
-37.865145	-2.007855	1.641574	0.007232	0.703333
-38.137357	-1.958790	1.646579	0.007283	0.703334
-37.794400	-2.017317	1.651584	0.007219	0.703339
-38.275393	-2.090166	1.656589	0.007309	0.703019
-38.800188	-2.004102	1.661594	0.007406	0.703004
-39.154435	-1.945278	1.666598	0.007472	0.702995
-38.676448	-2.028271	1.671603	0.007383	0.702999
-38.802495	-2.004801	1.676608	0.007407	0.703001
-39.170700	-1.941363	1.681613	0.007475	0.702997
-38.515982	-2.053432	1.686618	0.007353	0.703006
-38.978024	-2.102502	1.691622	0.007439	0.702741
-39.975509	-1.952044	1.696627	0.007625	0.702686
-39.718692	-1.995604	1.701632	0.007577	0.702690
-39.631572	-2.015589	1.706637	0.007561	0.702681
-39.860455	-1.969419	1.711642	0.007604	0.702692
-39.898234	-1.966285	1.716646	0.007611	0.702685
-39.504483	-2.033952	1.721651	0.007537	0.702690
-39.834279	-2.086845	1.726656	0.007599	0.702464
-41.273621	-1.880365	1.731661	0.007867	0.702363
-40.525860	-2.010270	1.736666	0.007728	0.702370
-40.459998	-2.025150	1.741670	0.007715	0.702363
-41.022587	-1.923418	1.746675	0.007820	0.702366
-40.559046	-2.003068	1.751680	0.007734	0.702372
-40.557900	-2.008880	1.756685	0.007733	0.702361
-40.795148	-2.025959	1.761690	0.007778	0.702241
-42.013282	-1.895100	1.766694	0.008004	0.702066
-41.165306	-2.046197	1.771699	0.007847	0.702067
-41.275549	-2.022998	1.776704	0.007867	0.702074
-41.840021	-1.927875	1.781709	0.007972	0.702063
-41.109717	-2.054015	1.786714	0.007836	0.702071
-41.340720	-2.015111	1.791718	0.007879	0.702066
-41.773285	-1.997914	1.796723	0.007960	0.701945
-42.471759	-1.972596	1.801728	0.008090	0.701744
-42.248615	-2.016831	1.806733	0.008048	0.701735
-42.380715	-1.987538	1.811738	0.008073	0.701747
-42.698371	-1.935765	1.816742	0.008132	0.701737
-42.369307	-1.992947	1.821747	0.008071	0.701740
-42.295209	-2.004009	1.826752	0.008057	0.701745
-42.788266	-1.922232	1.831757	0.008149	0.701732
-42.906506	-2.045034	1.836762	0.008171	0.701441
-43.139975	-2.008847	1.841766	0.008214	0.701430
-43.386801	-1.963417	1.846771	0.008260	0.701433
-43.035918	-2.024993	1.851776	0.008195	0.701435
-43.081717	-2.019264	1.856781	0.008203	0.701430
-43.065006	-2.018359	1.861786	0.008200	0.701438
-43.361193	-2.012277	1.866790	0.008255	0.701343
-44.141631	-1.983464	1.871795	0.008400	0.701120
-43.490636	-2.097556	1.876800	0.008279	0.701124
-44.078397	-1.996146	1.881805	0.008389	0.701117
-43.901563	-2.025030	1.886810	0.008356	0.701122
-43.736832	-2.057575	1.891814	0.008325	0.701116
-44.091700	-1.994303	1.896819	0.008391	0.701116
-44.243432	-2.062501	1.901824	0.008419	0.700923
-44.927447	-1.970235	1.906829	0.008547	0.700863
-44.620821	-2.018991	1.911834	0.008490	0.700875
-44.655240	-2.017216	1.916838	0.008496	0.700866
-44.725107	-2.003264	1.921843	0.008509	0.700869
-44.470156	-2.047197	1.926848	0.008462	0.700872
-44.942364	-2.035142	1.931853	0.008549	0.700726
-45.793461	-1.977604	1.936858	0.008708	0.700535
-45.206898	-2.085180	1.941862	0.008599	0.700529
-45.627592	-2.010052	1.946867	0.008677	0.700529
-45.678261	-1.998330	1.951872	0.008686	0.700535
-45.672431	-2.002421	1.956877	0.008685	0.700529
-45.449541	-2.038443	1.961882	0.008644	0.700536
-46.203007	-2.034391	1.966886	0.008784	0.700272
-46.801518	-1.956684	1.971891	0.008896	0.700213
-46.514515	-2.007529	1.976896	0.008842	0.700214
-46.508776	-2.011795	1.981901	0.008841	0.700207
-46.465223	-2.013260	1.986906	0.008833	0.700220
-46.325539	-2.041643	1.991910	0.008807	0.700213
-46.398319	-2.028481	1.996915	0.008820	0.700213
-47.283926	-2.022917	2.001920	0.008985	0.699904
-47.098851	-2.061295	2.011917	0.008951	0.699893
-47.179071	-2.047432	2.021914	0.008966	0.699893
-47.525625	-1.986225	2.031910	0.009030	0.699891
-47.257005	-2.034765	2.041907	0.008980	0.699890
-47.531842	-1.984460	2.051904	0.009031	0.699893
-47.160837	-2.050643	2.061901	0.008962	0.699893
-47.383831	-2.010432	2.071898	0.009004	0.699894
-47.444766	-2.001509	2.081894	0.009015	0.699890
-47.321359	-2.023998	2.091891	0.008992	0.699889
-47.300702	-2.027624	2.101888	0.008988	0.699889
-47.292458	-2.028073	2.111885	0.008987	0.699891
-47.482548	-1.994230	2.121882	0.009022	0.699891
-47.049702	-1.975797	2.131878	0.008941	0.700085
-46.367288	-2.035212	2.141875	0.008814	0.700212
-46.696791	-1.974273	2.151872	0.008876	0.700216
-46.255749	-2.052828	2.161869	0.008794	0.700216
-46.538889	-2.002277	2.171866	0.008846	0.700216
-46.215672	-1.993498	2.181862	0.008786	0.700351
-45.236648	-2.081109	2.191859	0.008604	0.700528
-45.585801	-2.017360	2.201856	0.008669	0.700531
-45.392010	-2.050241	2.211853	0.008633	0.700534
-45.600369	-2.013103	2.221850	0.008671	0.700534
-44.908166	-1.976766	2.231846	0.008543	0.700858
-44.756035	-1.997048	2.241843	0.008514	0.700872
-44.725198	-2.003183	2.251840	0.008508	0.700871
-44.550537	-2.021041	2.261837	0.008476	0.700897
-44.156759	-1.981447	2.271834	0.008403	0.701120
-43.866976	-2.033912	2.281830	0.008349	0.701118
-44.048116	-2.001475	2.291827	0.008382	0.701119
-43.718519	-1.971588	2.301824	0.008321	0.701298
-43.105698	-2.014224	2.311821	0.008207	0.701433
-43.318973	-1.976868	2.321818	0.008246	0.701432
-43.022924	-2.003080	2.331814	0.008191	0.701486
-42.178134	-2.029171	2.341811	0.008034	0.701738
-42.151744	-2.032390	2.351808	0.008029	0.701741
-42.104702	-2.041415	2.361805	0.008020	0.701740
-41.971316	-1.966721	2.371802	0.007995	0.701939
-41.323978	-2.016834	2.381798	0.007875	0.702071
-41.525664	-1.982435	2.391795	0.007912	0.702068
-41.369191	-1.980795	2.401792	0.007883	0.702128
-40.515167	-2.014283	2.411789	0.007724	0.702368
-40.645521	-1.991755	2.421786	0.007748	0.702367
-40.466322	-2.023417	2.431782	0.007715	0.702367
-40.058719	-1.969797	2.441779	0.007639	0.702623
-39.707982	-1.999056	2.451776	0.007574	0.702690
-39.412319	-2.050864	2.461773	0.007519	0.702692
-39.659259	-1.964810	2.471770	0.007565	0.702777
-38.683635	-2.027249	2.481766	0.007383	0.703002
-38.921843	-1.985414	2.491763	0.007427	0.703001
-38.690531	-2.025670	2.501760	0.007384	0.703003
-38.145537	-1.989495	2.511757	0.007283	0.703272
-37.953145	-1.989790	2.521754	0.007247	0.703341
-37.668457	-2.041457	2.531750	0.007194	0.703339
-37.893416	-1.969234	2.541747	0.007236	0.703404
-36.935187	-2.026988	2.551744	0.007057	0.703632
-37.015265	-2.012342	2.561741	0.007072	0.703633
-37.162722	-1.986806	2.571738	0.007100	0.703631
-36.519783	-1.972615	2.581734	0.006980	0.703891
-36.256541	-1.991049	2.591731	0.006931	0.703949
-36.007827	-2.036108	2.601728	0.006885	0.703947
-35.988313	-1.988687	2.611725	0.006881	0.704050
-35.270914	-2.014243	2.621722	0.006747	0.704257
-35.240412	-2.019235	2.631718	0.006742	0.704257
-35.616900	-1.954419	2.641715	0.006812	0.704253
-34.663995	-1.967442	2.651712	0.006634	0.704569
-34.376579	-2.010634	2.661709	0.006581	0.704585
-34.378868	-2.009663	2.671706	0.006581	0.704586
-34.207769	-1.968193	2.681702	0.006549	0.704732
-33.530900	-2.015439	2.691699	0.006423	0.704879
-33.590754	-2.005524	2.701696	0.006434	0.704878
-33.580938	-2.005314	2.711693	0.006432	0.704882
-32.911539	-1.965195	2.721690	0.006308	0.705203
-32.737135	-1.994830	2.731686	0.006275	0.705206
-32.782075	-1.986954	2.741683	0.006284	0.705206
-32.095832	-2.022962	2.751680	0.006156	0.705380
-31.884237	-1.990139	2.761677	0.006116	0.705522
-31.711442	-2.020768	2.771674	0.006084	0.705522
-31.773175	-2.010830	2.781670	0.006096	0.705520
-30.941393	-1.995616	2.791667	0.005941	0.705849
-30.910426	-1.995754	2.801664	0.005935	0.705860
-30.880565	-2.001173	2.811661	0.005929	0.705860
-30.925858	-1.932067	2.821658	0.005938	0.705982
-30.329600	-1.968100	2.831654	0.005827	0.706124
-30.358384	-1.963104	2.841651	0.005832	0.706123
-30.023929	-1.979591	2.851648	0.005770	0.706210
-29.349722	-1.985977	2.861645	0.005644	0.706439
-29.289701	-1.996150	2.871642	0.005633	0.706440
-29.345571	-1.987960	2.881638	0.005643	0.706436
-28.497308	-2.003894	2.891635	0.005486	0.706708
-28.407650	-2.000480	2.901632	0.005469	0.706747
-28.404284	-2.001332	2.911629	0.005468	0.706747
-28.244993	-1.967990	2.921626	0.005438	0.706871
-27.531105	-1.994529	2.931622	0.005306	0.707073
-27.615599	-1.979292	2.941619	0.005321	0.707073
-27.613377	-1.979162	2.951616	0.005321	0.707075
-27.095965	-1.928979	2.961613	0.005224	0.707360
-26.650115	-2.002238	2.971610	0.005141	0.707373
-26.723944	-1.989603	2.981606	0.005155	0.707372
-26.220605	-1.986481	2.991603	0.005061	0.707558
-25.925742	-1.970721	3.001600	0.005006	0.707695
-25.728968	-2.005033	3.011597	0.004970	0.707697
-25.770899	-1.983045	3.021594	0.004978	0.707726
-25.201004	-1.944998	3.031590	0.004871	0.708006
-24.607328	-2.050832	3.041587	0.004761	0.708006
-24.961418	-1.986686	3.051584	0.004827	0.708008
-24.673446	-1.957174	3.061581	0.004773	0.708170
-23.922118	-2.003675	3.071578	0.004633	0.708345
-24.124569	-1.966324	3.081574	0.004671	0.708348
-23.849258	-2.017245	3.091571	0.004620	0.708344
-23.383951	-1.957226	3.101568	0.004533	0.708631
-23.084838	-2.008136	3.111565	0.004477	0.708636
-23.083836	-2.006109	3.121562	0.004477	0.708640
-23.015844	-1.939459	3.131558	0.004464	0.708798
-22.129112	-2.021951	3.141555	0.004299	0.708949
-22.506612	-1.953597	3.151552	0.004370	0.708951
-22.119906	-2.019726	3.161549	0.004298	0.708957
-21.514716	-1.974233	3.171546	0.004185	0.709264
-21.364014	-2.002555	3.181542	0.004157	0.709261
-21.350138	-2.006179	3.191539	0.004154	0.709259
-21.327663	-1.931657	3.201536	0.004150	0.709416
-20.278078	-2.031609	3.211533	0.003954	0.709590
-20.518484	-1.987494	3.221530	0.003999	0.709593
-20.477897	-1.995098	3.231526	0.003992	0.709592
-19.940796	-1.952058	3.241523	0.003892	0.709870
-19.812876	-1.964398	3.251520	0.003868	0.709891
-19.338011	-2.049592	3.261517	0.003779	0.709889
-19.625093	-1.911852	3.271514	0.003833	0.710063
-18.848652	-1.975864	3.281510	0.003688	0.710211
-18.990898	-1.950494	3.291507	0.003715	0.710211
-18.663246	-1.988058	3.301504	0.003654	0.710253
-17.952744	-1.977502	3.311501	0.003521	0.710527
-17.751234	-2.011475	3.321498	0.003484	0.710531
-18.021987	-1.965435	3.331494	0.003534	0.710527
-17.369388	-1.972646	3.341491	0.003413	0.710744
-17.178712	-1.947655	3.351488	0.003377	0.710862
-16.785784	-2.014367	3.361485	0.003304	0.710869
-17.239352	-1.922950	3.371482	0.003388	0.710890
-16.216674	-1.983712	3.381478	0.003198	0.711132
-16.222292	-1.982377	3.391475	0.003199	0.711133
-16.321261	-1.966757	3.401472	0.003217	0.711129
-15.828961	-1.943146	3.411469	0.003126	0.711351
-15.625928	-1.929041	3.421466	0.003088	0.711452
-15.460517	-1.959593	3.431462	0.003057	0.711450
-15.289473	-1.922498	3.441459	0.003025	0.711584
-14.188280	-2.033965	3.451456	0.002820	0.711753
-14.143702	-2.040202	3.461453	0.002812	0.711757
-14.585778	-1.960389	3.471450	0.002894	0.711759
-13.678512	-1.995320	3.481446	0.002725	0.712012
-13.565700	-1.977677	3.491443	0.002704	0.712087
-13.316188	-2.022194	3.501440	0.002658	0.712087
-13.400706	-2.003937	3.511437	0.002673	0.712093
-12.646433	-1.992591	3.521434	0.002533	0.712384
-12.362735	-2.043395	3.531430	0.002480	0.712383
-12.771027	-1.971802	3.541427	0.002556	0.712381
-12.403756	-1.978994	3.551424	0.002488	0.712497
-11.305159	-2.068361	3.561421	0.002283	0.712709
-11.603731	-2.015808	3.571418	0.002339	0.712708
-11.534325	-2.029489	3.581414	0.002326	0.712705
-11.298127	-1.967164	3.591411	0.002282	0.712913
-10.499732	-2.055914	3.601408	0.002133	0.713019
-10.796988	-2.001320	3.611405	0.002188	0.713023
-10.520683	-2.050452	3.621402	0.002137	0.713023
-9.978778	-1.986640	3.631398	0.002036	0.713342
-9.649213	-2.039680	3.641395	0.001975	0.713353
-9.637512	-2.040291	3.651392	0.001972	0.713356
-9.724404	-1.983609	3.661389	0.001988	0.713438
-8.915166	-2.020712	3.671386	0.001838	0.713651
-8.801689	-2.042638	3.681382	0.001817	0.713648
-9.114207	-1.987213	3.691379	0.001875	0.713647
-8.253964	-2.014847	3.701376	0.001715	0.713897
-8.221768	-1.985525	3.711373	0.001709	0.713967
-7.892617	-2.043085	3.721370	0.001647	0.713969
-8.041067	-1.977170	3.731366	0.001675	0.714048
-7.069560	-2.037611	3.741363	0.001494	0.714271
-6.959065	-2.055860	3.751360	0.001473	0.714274
-7.004502	-2.046249	3.761357	0.001482	0.714277
-6.635035	-2.030639	3.771354	0.001413	0.714439
-6.059563	-2.050608	3.781350	0.001306	0.714603
-6.258113	-2.014428	3.791347	0.001343	0.714605
-5.924887	-2.074639	3.801344	0.001281	0.714603
-5.644636	-2.013328	3.811341	0.001229	0.714824
-5.207436	-2.047958	3.821338	0.001147	0.714910
-5.396054	-2.015477	3.831334	0.001182	0.714908
-5.266993	-1.993749	3.841331	0.001158	0.714996
-4.372997	-2.034658	3.851328	0.000992	0.715231
-4.573513	-1.998364	3.861325	0.001029	0.715232
-4.298023	-2.048091	3.871322	0.000978	0.715231
-3.689452	-2.030029	3.881318	0.000864	0.715482
-3.538128	-2.027404	3.891315	0.000836	0.715541
-3.355339	-2.058567	3.901312	0.000802	0.715543
-3.339574	-2.048268	3.911309	0.000799	0.715570
-2.420100	-2.055159	3.921306	0.000628	0.715881
-2.359157	-2.067967	3.931302	0.000617	0.715877
-2.478634	-2.046742	3.941299	0.000639	0.715877
-2.474002	-2.010474	3.951296	0.000638	0.715950
-1.773896	-2.044087	3.961293	0.000508	0.716131
-1.665799	-2.064269	3.971290	0.000487	0.716129
-1.711251	-2.055600	3.981286	0.000496	0.716130
-1.332604	-1.983304	3.991283	0.000425	0.716407
-1.077883	-2.008608	4.001280	0.000378	0.716447
-1.114977	-2.001111	4.011277	0.000385	0.716448
-1.202768	-1.869907	4.021274	0.000401	0.716677
-1.205127	-1.830693	4.031270	0.000401	0.716754
-0.838351	-1.851936	4.041267	0.000333	0.716841
-0.597024	-1.773129	4.051264	0.000288	0.717082
-0.608548	-1.769989	4.061261	0.000290	0.717085
-0.660165	-1.632479	4.071258	0.000300	0.717338
-0.654081	-1.613387	4.081254	0.000299	0.717378
-0.807810	-1.445737	4.091251	0.000327	0.717656
-0.597758	-1.446913	4.101248	0.000288	0.717727
-0.570301	-1.304346	4.111245	0.000283	0.718019
-0.259512	-1.293378	4.121242	0.000225	0.718150
-0.250874	-1.192134	4.131238	0.000223	0.718353
-0.349792	-1.061728	4.141235	0.000241	0.718576
-0.370573	-0.976922	4.151232	0.000245	0.718736
-0.304954	-0.875128	4.161229	0.000233	0.718960
-0.108536	-0.766599	4.171226	0.000196	0.719243
-0.142309	-0.653958	4.181222	0.000202	0.719453
-0.062525	-0.553224	4.191219	0.000187	0.719680
-0.148898	-0.417230	4.201216	0.000203	0.719918
-0.164461	-0.257901	4.211213	0.000206	0.720226
0.022951	-0.145645	4.221210	0.000171	0.720513
-0.087226	0.020696	4.231206	0.000192	0.720802
0.000000	0.149639	4.241203	0.000175	0.721086
0.058679	0.778944	4.246208	0.000164	0.722343
0.336792	2.001327	4.251213	0.000111	0.724837
0.523506	3.819457	4.256218	0.000075	0.728451
0.920495	6.170915	4.261222	-0.000000	0.733153
1.127750	9.049084	4.266227	-0.000041	0.738771
1.358359	12.408452	4.271232	-0.000086	0.745271
1.761017	16.197799	4.276237	-0.000163	0.752584
2.106775	20.389670	4.281242	-0.000230	0.760558
2.677757	24.951331	4.286246	-0.000340	0.769206
2.806949	29.951751	4.291251	-0.000367	0.778414
3.180771	35.256499	4.296256	-0.000440	0.788140
3.676519	40.861782	4.301261	-0.000536	0.798321
4.079748	46.774871	4.306266	-0.000615	0.808883
4.627906	52.957346	4.311270	-0.000721	0.819821
4.984250	59.439232	4.316275	-0.000792	0.831067
5.473320	66.121842	4.321280	-0.000887	0.842540
5.917548	73.039289	4.326285	-0.000974	0.854235
6.007098	80.208735	4.331290	-0.000996	0.866083
8.400247	87.185819	4.336294	-0.001446	0.878115
9.507057	94.581250	4.341299	-0.001657	0.890289
9.844347	102.276118	4.346304	-0.001725	0.902556
10.839168	110.002297	4.351309	-0.001915	0.914886
12.168893	117.786177	4.356314	-0.002167	0.927230
12.726373	125.846934	4.361318	-0.002277	0.939624
12.969623	134.046343	4.366323	-0.002327	0.951982
13.403819	142.290963	4.371328	-0.002413	0.964296
14.104366	150.579704	4.376333	-0.002549	0.976587
22.666370	157.676791	4.381338	-0.004148	0.988979
23.663343	166.206366	4.386342	-0.004339	1.001377
23.901030	174.874496	4.391347	-0.004389	1.013632
24.213753	183.551508	4.396352	-0.004453	1.025771
24.855368	192.203029	4.401357	-0.004578	1.037811
25.956192	200.782970	4.406362	-0.004789	1.049723
26.760231	209.456534	4.411366	-0.004944	1.061558
27.173666	218.193055	4.416371	-0.005027	1.073255
28.292530	226.803239	4.421376	-0.005241	1.084820
29.480337	235.429443	4.426381	-0.005468	1.096299
30.088266	244.142338	4.431386	-0.005587	1.107641
30.744648	252.862767	4.436390	-0.005714	1.118888
31.768335	261.497799	4.441395	-0.005911	1.129994
32.638874	270.168838	4.446400	-0.006078	1.141004
33.726757	278.819681	4.451405	-0.006287	1.151929
34.410401	287.496341	4.456410	-0.006420	1.162699
34.943866	296.184306	4.461414	-0.006525	1.173351
35.593025	304.818415	4.466419	-0.006651	1.183867
36.632951	313.395525	4.471424	-0.006850	1.194301
37.138542	322.040981	4.476429	-0.006950	1.204618
37.782570	330.648713	4.481434	-0.007076	1.214830
39.092270	339.146418	4.486438	-0.007325	1.224960
39.638128	347.775038	4.491443	-0.007432	1.235008
40.554330	356.285515	4.496448	-0.007609	1.244912
41.519650	364.806499	4.501453	-0.007794	1.254758
41.804401	373.397039	4.506458	-0.007852	1.264476
42.385716	381.950783	4.511462	-0.007966	1.274135
43.461449	390.379905	4.516467	-0.008172	1.283675
44.434048	398.846981	4.521472	-0.008359	1.293167
45.514056	407.288683	4.526477	-0.008565	1.302581
45.926751	415.894215	4.531482	-0.008648	1.311983
46.598570	424.392959	4.536486	-0.008778	1.321250
46.973586	432.853892	4.541491	-0.008854	1.330360
47.694200	441.257244	4.546496	-0.008993	1.339407
48.226592	449.680884	4.551501	-0.009098	1.348381
48.815438	458.084215	4.556506	-0.009213	1.357285
49.503863	466.456713	4.561510	-0.009347	1.366115
50.379860	474.808183	4.566515	-0.009515	1.374899
51.140859	483.158134	4.571520	-0.009663	1.383606
52.266543	491.485113	4.576525	-0.009878	1.392296
52.605638	499.889012	4.581530	-0.009946	1.400877
53.508113	508.206397	4.586534	-0.010120	1.409413
53.976365	516.587108	4.591539	-0.010212	1.417889
54.449600	524.930838	4.596544	-0.010306	1.426278
55.079340	533.282033	4.601549	-0.010429	1.434651
55.741476	541.578741	4.606554	-0.010557	1.442927
56.146553	549.936325	4.611558	-0.010638	1.451174
56.304779	558.316573	4.616563	-0.010673	1.459356
56.945142	566.600474	4.621568	-0.010798	1.467476
57.697869	574.930658	4.626573	-0.010943	1.475613
58.130094	583.203264	4.631578	-0.011029	1.483600
58.704453	591.486504	4.636582	-0.011142	1.491577
59.346726	599.736548	4.641587	-0.011267	1.499489
59.938975	607.991886	4.646592	-0.011382	1.507358
60.424273	616.286406	4.651597	-0.011478	1.515205
60.790779	624.548775	4.656602	-0.011552	1.522965
61.978124	632.711088	4.661606	-0.011778	1.530715
62.311736	641.016943	4.666611	-0.011846	1.538431
62.774182	649.275066	4.671616	-0.011937	1.546083
63.017693	657.598208	4.676621	-0.011988	1.553724
63.668819	665.792119	4.681626	-0.012115	1.561271
64.243219	674.023349	4.686630	-0.012227	1.568803
64.940723	682.234710	4.691635	-0.012362	1.576300
65.578602	690.437693	4.696640	-0.012486	1.583744
66.119902	698.681767	4.701645	-0.012592	1.591176
66.524413	706.926096	4.706650	-0.012673	1.598554
66.897050	715.156447	4.711654	-0.012748	1.605881
67.427621	723.381940	4.716659	-0.012852	1.613193
68.685667	731.476557	4.721664	-0.013092	1.620459
69.471759	739.680879	4.726669	-0.013243	1.627722
69.889082	747.977190	4.731674	-0.013326	1.634981
70.356289	756.194130	4.736678	-0.013419	1.642146
70.864579	764.389522	4.741683	-0.013519	1.649267
71.262526	772.611843	4.746688	-0.013598	1.656365
71.465586	780.844414	4.751693	-0.013641	1.663415
71.747584	789.048452	4.756698	-0.013699	1.670422
72.253403	797.242551	4.761702	-0.013799	1.677421
72.462011	805.439418	4.766707	-0.013843	1.684353
73.317146	813.556689	4.771712	-0.014008	1.691276
73.735436	821.754327	4.776717	-0.014091	1.698180
74.209953	829.907569	4.781722	-0.014184	1.705026
74.681133	838.119934	4.786726	-0.014278	1.711894
75.283082	846.266585	4.791731	-0.014395	1.718696
75.766759	854.413201	4.796736	-0.014490	1.725456
76.260868	862.603268	4.801741	-0.014588	1.732226
76.762341	870.762834	4.806746	-0.014686	1.738946
77.273939	878.916929	4.811750	-0.014787	1.745637
77.629351	887.117043	4.816755	-0.014858	1.752320
77.739764	895.328347	4.821760	-0.014884	1.758955
78.344840	903.442449	4.826765	-0.015002	1.765549
78.764862	911.605793	4.831770	-0.015086	1.772135
79.508694	919.730158	4.836774	-0.015230	1.778705
80.014452	927.861091	4.841779	-0.015329	1.785227
80.357742	936.079701	4.846784	-0.015398	1.791774
80.590037	944.288830	4.851789	-0.015447	1.798276
80.852848	952.413151	4.856794	-0.015501	1.804692
81.575626	960.523722	4.861798	-0.015641	1.811130
82.199807	968.634196	4.866803	-0.015763	1.817533
82.200604	976.830990	4.871808	-0.015768	1.823905
82.828127	984.957754	4.876813	-0.015890	1.830276
83.098423	993.125453	4.881818	-0.015946	1.836614
83.880582	1001.203599	4.886822	-0.016097	1.842922
84.240010	1009.360540	4.891827	-0.016169	1.849218
85.017781	1017.455157	4.896832	-0.016319	1.855494
85.778213	1025.543208	4.901837	-0.016466	1.861742
86.352604	1033.670274	4.906842	-0.016578	1.867977
86.959727	1041.837620	4.911846	-0.016697	1.874225
87.399256	1049.961073	4.916851	-0.016784	1.880400
87.736073	1058.105436	4.921856	-0.016852	1.886558
88.160750	1066.271111	4.926861	-0.016936	1.892723
88.461450	1074.401163	4.931866	-0.016998	1.898826
88.920609	1082.526290	4.936870	-0.017088	1.904924
89.377256	1090.657819	4.941875	-0.017179	1.911007
89.903709	1098.781870	4.946880	-0.017282	1.917073
90.540143	1106.871832	4.951885	-0.017406	1.923106
90.640390	1115.040347	4.956890	-0.017430	1.929119
91.320305	1123.138398	4.961894	-0.017562	1.935126
91.339898	1131.315089	4.966899	-0.017571	1.941098
91.960910	1139.391432	4.971904	-0.017692	1.947045
92.475924	1147.550074	4.976909	-0.017793	1.953022
92.692534	1155.682075	4.981914	-0.017839	1.958929
92.975470	1163.782739	4.986918	-0.017897	1.964802
93.512802	1171.869235	4.991923	-0.018002	1.970675
94.262880	1179.941822	4.996928	-0.018147	1.976544
94.877104	1188.030433	5.001933	-0.018266	1.982391
95.226186	1196.147177	5.006938	-0.018337	1.988214
95.688029	1204.285784	5.011942	-0.018428	1.994046
95.878052	1212.409112	5.016947	-0.018469	1.999822
96.035310	1220.533526	5.021952	-0.018503	2.005579
96.505560	1228.653954	5.026957	-0.018596	2.011349
96.963388	1236.756996	5.031962	-0.018687	2.017089
97.371342	1244.842675	5.036966	-0.018768	2.022795
97.835785	1252.936269	5.041971	-0.018860	2.028496
98.212436	1261.078977	5.046976	-0.018935	2.034206
98.680607	1269.155361	5.051981	-0.019028	2.039864
98.766828	1277.263044	5.056986	-0.019049	2.045488
99.608842	1285.313277	5.061990	-0.019211	2.051134
100.118073	1293.408353	5.066995	-0.019311	2.056762
100.517217	1301.496163	5.072000	-0.019391	2.062358
100.971090	1309.604442	5.077005	-0.019481	2.067958
101.297948	1317.736679	5.082010	-0.019547	2.073547
101.696025	1325.837630	5.087014	-0.019626	2.079106
102.036462	1333.926197	5.092019	-0.019695	2.084637
102.191061	1342.052690	5.097024	-0.019729	2.090159
103.011564	1350.111132	5.102029	-0.019887	2.095687
103.230773	1358.215340	5.107034	-0.019933	2.101172
103.636404	1366.309751	5.112038	-0.020014	2.106654
104.169398	1374.436307	5.117043	-0.020118	2.112156
104.319440	1382.578991	5.122048	-0.020152	2.117617
104.985943	1390.599992	5.127053	-0.020281	2.123033
105.595845	1398.633703	5.132058	-0.020400	2.128438
106.074492	1406.750504	5.137062	-0.020494	2.133871
106.125373	1414.874462	5.142067	-0.020509	2.139255
106.522816	1422.935663	5.147072	-0.020588	2.144616
106.964606	1431.039949	5.152077	-0.020676	2.149996
107.261027	1439.135001	5.157082	-0.020736	2.155344
107.511588	1447.234050	5.162086	-0.020788	2.160676
107.866926	1455.303715	5.167091	-0.020860	2.165985
108.552729	1463.358881	5.172096	-0.020993	2.171303
108.830820	1471.486990	5.177101	-0.021050	2.176617
109.041306	1479.566766	5.182106	-0.021094	2.181881
109.710569	1487.613259	5.187110	-0.021224	2.187153
109.953983	1495.744309	5.192115	-0.021275	2.192427
110.493322	1503.801883	5.197120	-0.021380	2.197668
110.993934	1511.855638	5.202125	-0.021479	2.202891
111.050946	1519.968021	5.207130	-0.021495	2.208098
111.452744	1528.059383	5.212134	-0.021575	2.213311
111.860494	1536.124972	5.217139	-0.021656	2.218496
112.208544	1544.188668	5.222144	-0.021726	2.223662
112.383948	1552.308128	5.227149	-0.021764	2.228836
112.798005	1560.386805	5.232154	-0.021846	2.233993
113.325944	1568.436168	5.237158	-0.021950	2.239130
113.537851	1576.512108	5.242163	-0.021995	2.244244
113.962476	1584.578719	5.247168	-0.022079	2.249359
114.294169	1592.712278	5.252173	-0.022146	2.254496
114.451918	1600.767606	5.257178	-0.022181	2.259557
114.691829	1608.860960	5.262182	-0.022231	2.264638
115.171961	1616.938875	5.267187	-0.022325	2.269718
115.895657	1625.028396	5.272192	-0.022465	2.274815
116.344707	1633.068094	5.277197	-0.022554	2.279847
116.599099	1641.128028	5.282202	-0.022607	2.284862
117.000125	1649.190962	5.287206	-0.022687	2.289881
117.368591	1657.271292	5.292211	-0.022761	2.294897
117.711314	1665.318778	5.297216	-0.022830	2.299880
118.380873	1673.359211	5.302221	-0.022960	2.304875
118.653003	1681.452136	5.307226	-0.023016	2.309858
118.929014	1689.570126	5.312230	-0.023072	2.314845
119.012506	1697.654541	5.317235	-0.023093	2.319785
119.448133	1705.685884	5.322240	-0.023180	2.324712
119.714991	1713.784315	5.327245	-0.023235	2.329655
120.554330	1721.805498	5.332250	-0.023396	2.334588
121.196615	1729.857572	5.337254	-0.023521	2.339512
121.387959	1737.940356	5.342259	-0.023562	2.344408
121.577669	1746.044548	5.347264	-0.023602	2.349306
122.318515	1754.133087	5.352269	-0.023746	2.354230
122.950223	1762.142082	5.357274	-0.023869	2.359086
123.192088	1770.206765	5.362278	-0.023919	2.363934
123.541158	1778.282106	5.367283	-0.023989	2.368788
123.909731	1786.354336	5.372288	-0.024063	2.373630
124.129592	1794.444635	5.377293	-0.024109	2.378462
124.300480	1802.507063	5.382298	-0.024146	2.383264
124.763703	1810.558069	5.387302	-0.024238	2.388072
125.087218	1818.640865	5.392307	-0.024303	2.392878
125.380270	1826.702906	5.397312	-0.024363	2.397660
126.114645	1834.720557	5.402317	-0.024505	2.402441
126.405764	1842.788692	5.407322	-0.024565	2.407207
126.721682	1850.882240	5.412326	-0.024629	2.411980
127.153817	1858.956869	5.417331	-0.024714	2.416742
127.690477	1866.988413	5.422336	-0.024820	2.421477
128.072096	1875.068343	5.427341	-0.024896	2.426219
128.396651	1883.156848	5.432346	-0.024962	2.430953
128.686392	1891.289333	5.437350	-0.025021	2.435700
129.054763	1899.310574	5.442355	-0.025095	2.440379
129.431843	1907.310134	5.447360	-0.025170	2.445037
129.994695	1915.369781	5.452365	-0.025280	2.449736
130.290052	1923.435907	5.457370	-0.025341	2.454408
130.546521	1931.508305	5.462374	-0.025394	2.459072
130.940767	1939.550982	5.467379	-0.025472	2.463721
131.132497	1947.617018	5.472384	-0.025513	2.468359
131.514447	1955.703326	5.477389	-0.025590	2.473014
131.747930	1963.760154	5.482394	-0.025638	2.477633
131.971671	1971.819458	5.487398	-0.025685	2.482243
132.358896	1979.877077	5.492403	-0.025763	2.486856
132.332538	1987.980667	5.497408	-0.025763	2.491456
132.840985	1996.022590	5.502413	-0.025863	2.496052
133.132977	2004.050740	5.507418	-0.025923	2.500615
133.534357	2012.109794	5.512422	-0.026003	2.505196
133.798294	2020.181885	5.517427	-0.026057	2.509765
134.274001	2028.248014	5.522432	-0.026151	2.514338
134.449292	2036.317362	5.527437	-0.026189	2.518883
134.646436	2044.355962	5.532442	-0.026231	2.523404
135.028505	2052.389904	5.537446	-0.026307	2.527928
135.526272	2060.440476	5.542451	-0.026405	2.532460
135.702018	2068.499817	5.547456	-0.026443	2.536967
136.254999	2076.542658	5.552461	-0.026551	2.541483
136.700855	2084.563173	5.557466	-0.026639	2.545971
136.892982	2092.668948	5.562470	-0.026680	2.550481
137.305071	2100.722356	5.567475	-0.026762	2.554969
137.672603	2108.743816	5.572480	-0.026836	2.559428
137.841634	2116.813094	5.577485	-0.026873	2.563892
138.020882	2124.889869	5.582490	-0.026912	2.568352
138.328124	2132.958418	5.587494	-0.026974	2.572810
138.679204	2141.013721	5.592499	-0.027045	2.577255
138.941086	2149.051591	5.597504	-0.027099	2.581677
139.375500	2157.092617	5.602509	-0.027185	2.586105
139.640089	2165.184424	5.607514	-0.027239	2.590542
140.021387	2173.400933	5.612518	-0.027316	2.595046
140.190077	2181.402969	5.617523	-0.027352	2.599412
140.430353	2189.371390	5.622528	-0.027402	2.603757
140.910791	2197.395397	5.627533	-0.027497	2.608141
141.023942	2205.449419	5.632538	-0.027523	2.612509
141.466019	2213.490341	5.637542	-0.027611	2.616884
141.837596	2221.501324	5.642547	-0.027685	2.621232
141.883602	2229.551321	5.647552	-0.027699	2.625571
142.299701	2237.607888	5.652557	-0.027782	2.629931
142.691427	2245.655772	5.657562	-0.027860	2.634278
142.986007	2253.696799	5.662566	-0.027920	2.638608
143.253939	2261.742814	5.667571	-0.027975	2.642931
143.563359	2269.769298	5.672576	-0.028038	2.647239
143.901307	2277.848611	5.677581	-0.028106	2.651571
144.027430	2285.935279	5.682586	-0.028135	2.655885
144.321155	2293.962399	5.687590	-0.028195	2.660171
144.743919	2301.993387	5.692595	-0.028279	2.664461
144.894886	2310.058875	5.697600	-0.028312	2.668745
145.582205	2318.130101	5.702605	-0.028446	2.673059
146.006932	2326.154367	5.707610	-0.028530	2.677325
146.361922	2334.181176	5.712614	-0.028601	2.681580
146.746015	2342.228113	5.717619	-0.028678	2.685842
147.003484	2350.246888	5.722624	-0.028731	2.690073
147.452974	2358.336854	5.727629	-0.028820	2.694348
147.507571	2366.402208	5.732634	-0.028836	2.698577
147.739479	2374.437446	5.737638	-0.028884	2.702796
148.037337	2382.477467	5.742643	-0.028945	2.707014
148.031442	2390.546829	5.747648	-0.028949	2.711222
148.261639	2398.617896	5.752653	-0.028997	2.715440
148.631318	2406.606273	5.757658	-0.029071	2.719616
149.173361	2414.615491	5.762662	-0.029177	2.723807
149.438687	2422.679944	5.767667	-0.029232	2.728003
149.680449	2430.725362	5.772672	-0.029282	2.732182
150.040609	2438.806083	5.777677	-0.029355	2.736379
150.298142	2446.851627	5.782682	-0.029408	2.740546
150.764119	2454.845502	5.787686	-0.029500	2.744692
151.306502	2462.896175	5.792691	-0.029606	2.748866
151.660206	2471.021181	5.797696	-0.029677	2.753060
151.739888	2479.105113	5.802701	-0.029697	2.757210
151.911407	2487.122148	5.807706	-0.029734	2.761325
152.199153	2495.121119	5.812710	-0.029793	2.765432
152.452168	2503.162533	5.817715	-0.029846	2.769552
152.882397	2511.201492	5.822720	-0.029931	2.773675
153.349787	2519.240964	5.827725	-0.030023	2.777795
153.341135	2527.300748	5.832730	-0.030027	2.781890
153.666009	2535.328090	5.837734	-0.030093	2.785983
154.256207	2543.344027	5.842739	-0.030208	2.790079
154.649216	2551.380732	5.847744	-0.030286	2.794169
154.884151	2559.468135	5.852749	-0.030335	2.798268
155.023439	2567.472058	5.857754	-0.030366	2.802314
155.334424	2575.496988	5.862758	-0.030430	2.806374
155.605416	2583.589258	5.867763	-0.030485	2.810460
155.883098	2591.619296	5.872768	-0.030542	2.814510
156.337783	2599.658197	5.877773	-0.030632	2.818568
156.388547	2607.710908	5.882778	-0.030647	2.822604
156.377142	2615.797281	5.887782	-0.030650	2.826647
156.774222	2623.846113	5.892787	-0.030729	2.830689
157.045108	2631.894115	5.897792	-0.030785	2.834718
157.339585	2639.915904	5.902797	-0.030845	2.838729
157.533556	2647.925436	5.907802	-0.030886	2.842722
158.016700	2655.943770	5.912806	-0.030982	2.846731
158.260213	2664.008985	5.917811	-0.031032	2.850744
158.362239	2672.075187	5.922816	-0.031056	2.854743
158.747418	2680.099986	5.927821	-0.031133	2.858733
158.900509	2688.127536	5.932826	-0.031167	2.862705
159.513881	2696.127912	5.937830	-0.031287	2.866683
159.820321	2704.197653	5.942835	-0.031349	2.870674
160.188724	2712.224839	5.947840	-0.031423	2.874641
160.430683	2720.285092	5.952845	-0.031473	2.878612
160.595845	2728.325680	5.957850	-0.031509	2.882563
161.010600	2736.347043	5.962854	-0.031591	2.886513
161.257585	2744.404673	5.967859	-0.031643	2.890467
161.319026	2752.456962	5.972864	-0.031659	2.894402
161.808337	2760.502313	5.977869	-0.031756	2.898352
162.349413	2768.488389	5.982874	-0.031862	2.902270
162.656591	2776.541576	5.987878	-0.031924	2.906203
163.072029	2784.592627	5.992883	-0.032007	2.910135
163.220726	2792.737613	5.997888	-0.032040	2.914093
163.440161	2800.769884	6.002893	-0.032086	2.917995
163.696426	2808.739880	6.007898	-0.032139	2.921863
164.313265	2816.719284	6.012902	-0.032259	2.925750
164.565164	2824.765046	6.017907	-0.032311	2.929645
164.887580	2832.824991	6.022912	-0.032376	2.933544
165.099864	2840.875361	6.027917	-0.032421	2.937428
165.497542	2848.880600	6.032922	-0.032500	2.941295
165.732503	2856.915544	6.037926	-0.032549	2.945163
166.044747	2864.973679	6.042931	-0.032613	2.949040
166.347107	2873.003839	6.047936	-0.032674	2.952899
166.594518	2881.078053	6.052941	-0.032726	2.956770
166.900055	2889.076222	6.057946	-0.032788	2.960604
167.233735	2897.087800	6.062950	-0.032855	2.964440
167.582869	2905.156186	6.067955	-0.032925	2.968298
167.676248	2913.204172	6.072960	-0.032948	2.972129
167.910696	2921.288312	6.077965	-0.032997	2.975980
168.260193	2929.279204	6.082970	-0.033067	2.979787
168.409902	2937.337406	6.087974	-0.033100	2.983611
168.731092	2945.384499	6.092979	-0.033166	2.987433
168.902872	2953.424201	6.097984	-0.033203	2.991239
169.195276	2961.480668	6.102989	-0.033262	2.995055
169.379230	2969.492732	6.107994	-0.033302	2.998839
169.881151	2977.475491	6.112998	-0.033401	3.002620
170.350694	2985.521182	6.118003	-0.033493	3.006425
170.587248	2993.549899	6.123008	-0.033543	3.010205
171.363593	3001.586175	6.128013	-0.033692	3.014010
171.690116	3009.621418	6.133018	-0.033758	3.017788
171.721328	3017.676402	6.138022	-0.033769	3.021556
171.877810	3025.727054	6.143027	-0.033804	3.025323
172.323417	3033.736284	6.148032	-0.033892	3.029081
172.747272	3041.777406	6.153037	-0.033976	3.032847
172.743807	3049.859663	6.158042	-0.033981	3.036607
173.048248	3057.871651	6.163046	-0.034043	3.040345
173.475133	3065.881677	6.168051	-0.034128	3.044083
173.559530	3073.920941	6.173056	-0.034148	3.047813
173.862882	3081.989391	6.178061	-0.034210	3.051563
174.035710	3090.029326	6.183066	-0.034248	3.055289
174.207898	3098.046092	6.188070	-0.034285	3.058999
174.511468	3106.067360	6.193075	-0.034347	3.062714
174.698428	3114.096208	6.198080	-0.034387	3.066421
174.843944	3122.169654	6.203085	-0.034419	3.070143
175.184267	3130.263054	6.208090	-0.034488	3.073879
175.650068	3138.247564	6.213094	-0.034580	3.077565
175.970955	3146.276351	6.218099	-0.034645	3.081261
175.987990	3154.253610	6.223104	-0.034653	3.084915
176.325890	3162.313108	6.228109	-0.034721	3.088617
176.686742	3170.330904	6.233114	-0.034794	3.092296
176.820936	3178.394261	6.238118	-0.034824	3.095981
176.848901	3186.437528	6.243123	-0.034834	3.099648
177.187090	3194.448260	6.248128	-0.034903	3.103310
177.611305	3202.476515	6.253133	-0.034987	3.106979
177.393836	3210.559303	6.258138	-0.034952	3.110640
177.626728	3218.586648	6.263142	-0.035000	3.114291
177.989013	3226.614117	6.268147	-0.035073	3.117944
178.051806	3234.631910	6.273152	-0.035090	3.121575
178.584860	3242.626995	6.278157	-0.035194	3.125212
178.800310	3250.682454	6.283162	-0.035240	3.128859
179.018717	3258.701411	6.288166	-0.035286	3.132484
179.466416	3266.752967	6.293171	-0.035374	3.136130
180.077852	3274.723037	6.298176	-0.035493	3.139743
180.340026	3282.767455	6.303181	-0.035547	3.143369
180.414025	3290.813276	6.308186	-0.035566	3.146983
180.838667	3298.835523	6.313190	-0.035651	3.150598
181.078457	3306.954295	6.318195	-0.035701	3.154244
181.216713	3314.931134	6.323200	-0.035732	3.157818
181.449983	3322.988965	6.328205	-0.035780	3.161428
181.838896	3330.953541	6.333210	-0.035858	3.164999
182.281241	3338.996431	6.338214	-0.035946	3.168603
182.747708	3347.041467	6.343219	-0.036038	3.172205
182.999320	3355.109564	6.348224	-0.036090	3.175804
183.308295	3363.109701	6.353229	-0.036153	3.179370
183.520533	3371.147273	6.358234	-0.036197	3.182946
183.826667	3379.173022	6.363238	-0.036260	3.186516
184.495243	3387.183879	6.368243	-0.036389	3.190090
184.795532	3395.240598	6.373248	-0.036450	3.193666
185.103527	3403.288795	6.378253	-0.036513	3.197234
185.449607	3411.301461	6.383258	-0.036583	3.200783
185.684274	3419.285562	6.388262	-0.036632	3.204312
185.766695	3427.399425	6.393267	-0.036652	3.207887
185.966976	3435.435962	6.398272	-0.036695	3.211429
186.158109	3443.466695	6.403277	-0.036736	3.214965
186.221141	3451.494917	6.408282	-0.036753	3.218490
186.402061	3459.513079	6.413286	-0.036792	3.222011
186.955727	3467.502362	6.418291	-0.036900	3.225532
187.293876	3475.539358	6.423296	-0.036968	3.229060
187.534058	3483.635926	6.428301	-0.037018	3.232607
187.895651	3491.685118	6.433306	-0.037091	3.236134
188.017724	3499.660161	6.438310	-0.037119	3.239615
188.256645	3507.682527	6.443315	-0.037168	3.243117
188.237071	3515.733994	6.448320	-0.037170	3.246618
188.831399	3523.715231	6.453325	-0.037286	3.250110
189.149611	3531.774671	6.458330	-0.037350	3.253620
189.404417	3539.776026	6.463334	-0.037403	3.257099
189.952071	3547.798898	6.468339	-0.037510	3.260595
190.262009	3555.804738	6.473344	-0.037573	3.264070
190.418708	3563.871568	6.478349	-0.037608	3.267562
190.730324	3571.925765	6.483354	-0.037671	3.271051
190.998317	3579.954290	6.488358	-0.037726	3.274523
191.369570	3587.994439	6.493363	-0.037800	3.278001
191.471979	3595.988509	6.498368	-0.037825	3.281445
191.856951	3603.993861	6.503373	-0.037902	3.284900
192.120013	3612.042830	6.508378	-0.037956	3.288366
192.192555	3620.093520	6.513382	-0.037975	3.291822
192.552285	3628.154654	6.518387	-0.038047	3.295290
192.726560	3636.143993	6.523392	-0.038084	3.298716
193.008867	3644.181030	6.528397	-0.038142	3.302163
193.341497	3652.211885	6.533402	-0.038209	3.305605
193.463828	3660.232641	6.538406	-0.038237	3.309032
193.656392	3668.314910	6.543411	-0.038279	3.312484
193.669240	3676.362195	6.548416	-0.038286	3.315911
194.001660	3684.336709	6.553421	-0.038353	3.319315
194.345773	3692.346481	6.558426	-0.038423	3.322731
194.459038	3700.382764	6.563430	-0.038449	3.326146
194.903758	3708.394598	6.568435	-0.038537	3.329560
195.135510	3716.440896	6.573440	-0.038585	3.332977
195.385191	3724.499171	6.578445	-0.038637	3.336396
195.545432	3732.519689	6.583450	-0.038672	3.339792
195.702504	3740.510264	6.588454	-0.038707	3.343172
196.232148	3748.558870	6.593459	-0.038811	3.346586
196.388591	3756.575627	6.598464	-0.038845	3.349970
196.529660	3764.639742	6.603469	-0.038877	3.353370
196.890059	3772.674643	6.608474	-0.038949	3.356762
196.949524	3780.655251	6.613478	-0.038965	3.360117
197.381963	3788.702668	6.618483	-0.039051	3.363510
197.735856	3796.706291	6.623488	-0.039122	3.366878
197.834971	3804.747325	6.628493	-0.039146	3.370250
197.901666	3812.814157	6.633498	-0.039163	3.373627
198.339593	3820.824669	6.638502	-0.039250	3.376991
198.582643	3828.857671	6.643507	-0.039301	3.380354
198.698612	3836.858634	6.648512	-0.039328	3.383696
199.129427	3844.876210	6.653517	-0.039413	3.387053
199.473555	3852.922758	6.658522	-0.039482	3.390415
199.643218	3861.050707	6.663526	-0.039519	3.393801
199.824991	3869.068570	6.668531	-0.039558	3.397139
200.056712	3877.011221	6.673536	-0.039607	3.400444
200.208479	3885.020360	6.678541	-0.039640	3.403770
200.357005	3893.049747	6.683546	-0.039673	3.407102
200.443298	3901.074880	6.688550	-0.039694	3.410426
201.127999	3909.096826	6.693555	-0.039827	3.413766
201.144370	3917.133063	6.698560	-0.039835	3.417086
201.246131	3925.177657	6.703565	-0.039860	3.420409
201.529041	3933.169761	6.708570	-0.039917	3.423714
201.688134	3941.188991	6.713574	-0.039952	3.427022
202.021872	3949.251093	6.718579	-0.040020	3.430350
202.100903	3957.270570	6.723584	-0.040040	3.433649
202.600689	3965.324357	6.728589	-0.040138	3.436973
202.689324	3973.316831	6.733594	-0.040160	3.440255
203.060478	3981.317692	6.738598	-0.040234	3.443546
203.405997	3989.374996	6.743603	-0.040304	3.446857
203.368098	3997.384885	6.748608	-0.040302	3.450132
203.653168	4005.455852	6.753613	-0.040360	3.453440
203.860362	4013.497347	6.758618	-0.040404	3.456730
203.916133	4021.492886	6.763622	-0.040420	3.459993
204.307306	4029.522844	6.768627	-0.040498	3.463278
204.501288	4037.551792	6.773632	-0.040539	3.466553
204.867102	4045.570151	6.778637	-0.040612	3.469826
204.930799	4053.640222	6.783642	-0.040629	3.473107
205.166401	4061.686656	6.788646	-0.040679	3.476382
205.625297	4069.619186	6.793651	-0.040769	3.479613
205.936394	4077.645728	6.798656	-0.040832	3.482876
206.120777	4085.677560	6.803661	-0.040872	3.486133
206.736375	4093.697094	6.808666	-0.040992	3.489396
206.948441	4101.731244	6.813670	-0.041037	3.492648
207.365608	4109.752349	6.818675	-0.041119	3.495899
207.682766	4117.764891	6.823680	-0.041184	3.499141
207.952991	4125.821994	6.828685	-0.041239	3.502395
208.347807	4133.832849	6.833690	-0.041318	3.505632
208.541204	4141.852869	6.838694	-0.041359	3.508863
209.130166	4149.874012	6.843699	-0.041474	3.512104
209.267967	4157.921163	6.848704	-0.041505	3.515339
209.521305	4165.922547	6.853709	-0.041558	3.518555
209.720792	4173.972912	6.858714	-0.041600	3.521787
209.964897	4181.947779	6.863718	-0.041651	3.524987
210.090710	4190.021793	6.868723	-0.041679	3.528220
210.429834	4198.053483	6.873728	-0.041748	3.531439
210.714762	4206.082682	6.878733	-0.041806	3.534653
210.751219	4214.147474	6.883738	-0.041818	3.537870
210.961388	4222.150902	6.888742	-0.041862	3.541066
211.457405	4230.144127	6.893747	-0.041960	3.544263
211.495173	4238.197175	6.898752	-0.041972	3.547467
211.750026	4246.237387	6.903757	-0.042025	3.550669
212.145522	4254.357114	6.908762	-0.042104	3.553905
212.407125	4262.329010	6.913766	-0.042158	3.557074
212.534807	4270.299150	6.918771	-0.042187	3.560237
212.764111	4278.288653	6.923776	-0.042235	3.563407
213.189318	4286.329371	6.928781	-0.042319	3.566600
213.329622	4294.357344	6.933786	-0.042351	3.569777
213.440893	4302.379639	6.938790	-0.042376	3.572948
213.701496	4310.457577	6.943795	-0.042430	3.576142
213.802027	4318.411904	6.948800	-0.042454	3.579281
213.956238	4326.463739	6.953805	-0.042488	3.582456
214.103745	4334.477241	6.958810	-0.042521	3.585613
214.224755	4342.464043	6.963814	-0.042549	3.588756
214.488703	4350.540637	6.968819	-0.042603	3.591936
214.671561	4358.588961	6.973824	-0.042642	3.595100
214.997541	4366.569668	6.978829	-0.042708	3.598238
214.932638	4374.630118	6.983834	-0.042701	3.601394
215.010343	4382.560554	6.988838	-0.042721	3.604500
215.467109	4390.633831	6.993843	-0.042811	3.607670
215.784587	4398.614787	6.998848	-0.042876	3.610797
215.908553	4406.692520	7.003853	-0.042904	3.613953
216.240426	4414.741082	7.008858	-0.042971	3.617101
216.387316	4422.706438	7.013862	-0.043004	3.620209
216.730401	4430.762809	7.018867	-0.043073	3.623355
216.781164	4438.797026	7.023872	-0.043088	3.626482
217.125086	4446.801671	7.028877	-0.043157	3.629603
217.305767	4454.895509	7.033882	-0.043196	3.632750
217.436522	4462.904929	7.038886	-0.043225	3.635862
217.785669	4470.913410	7.043891	-0.043296	3.638975
218.049896	4478.925099	7.048896	-0.043350	3.642086
218.261052	4486.912710	7.053901	-0.043394	3.645182
218.364574	4494.963068	7.058906	-0.043419	3.648298
218.635094	4503.003274	7.063910	-0.043475	3.651411
218.760547	4511.060369	7.068915	-0.043503	3.654524
219.002481	4519.056542	7.073920	-0.043554	3.657614
219.355879	4527.070672	7.078925	-0.043625	3.660712
219.527483	4535.100809	7.083930	-0.043662	3.663808
219.816710	4543.095786	7.088934	-0.043721	3.666891
220.075280	4551.144385	7.093939	-0.043774	3.669991
219.966449	4559.199341	7.098944	-0.043759	3.673081
220.289041	4567.212651	7.103949	-0.043825	3.676164
220.451807	4575.200318	7.108954	-0.043860	3.679231
220.591690	4583.214187	7.113958	-0.043891	3.682304
221.084725	4591.198352	7.118963	-0.043988	3.685372
220.980792	4599.253358	7.123968	-0.043974	3.688450
221.366214	4607.272176	7.128973	-0.044051	3.691524
221.538105	4615.302887	7.133978	-0.044088	3.694594
221.651240	4623.323741	7.138982	-0.044115	3.697656
222.055006	4631.356083	7.143987	-0.044195	3.700728
222.355982	4639.317501	7.148992	-0.044256	3.703767
222.427902	4647.377631	7.153997	-0.044275	3.706836
222.606014	4655.419531	7.159002	-0.044314	3.709897
223.095598	4663.491636	7.164006	-0.044410	3.712976
223.175136	4671.597872	7.169011	-0.044430	3.716054
223.319917	4679.514791	7.174016	-0.044462	3.719060
223.587752	4687.506147	7.179021	-0.044517	3.722095
223.935469	4695.511431	7.184026	-0.044587	3.725134
223.951963	4703.516397	7.189030	-0.044596	3.728163
224.241324	4711.570087	7.194035	-0.044655	3.731214
224.606840	4719.580210	7.199040	-0.044728	3.734248
224.650846	4727.636300	7.204045	-0.044741	3.737289
224.751874	4735.650670	7.209050	-0.044765	3.740313
224.946780	4743.640002	7.214054	-0.044807	3.743328
225.378692	4751.707366	7.219059	-0.044893	3.746375
225.360909	4759.699859	7.224064	-0.044895	3.749381
225.659407	4767.733171	7.229069	-0.044955	3.752407
225.963800	4775.796030	7.234074	-0.045017	3.755442
225.878352	4783.749734	7.239078	-0.045007	3.758424
226.336723	4791.817106	7.244083	-0.045097	3.761459
226.778290	4799.783015	7.249088	-0.045185	3.764454
226.952335	4807.849392	7.254093	-0.045222	3.767477
227.140329	4815.897267	7.259098	-0.045263	3.770491
227.239765	4823.895198	7.264102	-0.045286	3.773483
227.522616	4831.945314	7.269107	-0.045344	3.776495
227.583589	4839.936672	7.274112	-0.045361	3.779478
227.843391	4847.962648	7.279117	-0.045414	3.782476
228.047217	4855.978341	7.284122	-0.045458	3.785467
228.174136	4864.021000	7.289126	-0.045487	3.788463
228.691765	4872.051893	7.294131	-0.045588	3.791462
228.951212	4880.081990	7.299136	-0.045642	3.794451
229.102855	4888.103882	7.304141	-0.045675	3.797434
229.193795	4896.126468	7.309146	-0.045697	3.800412
229.550416	4904.058089	7.314150	-0.045769	3.803361
229.908464	4912.135893	7.319155	-0.045841	3.806361
230.142449	4920.112717	7.324160	-0.045890	3.809319
230.251582	4928.206967	7.329165	-0.045915	3.812315
230.439424	4936.216038	7.334170	-0.045955	3.815279
230.559794	4944.220943	7.339174	-0.045983	3.818238
230.815165	4952.232815	7.344179	-0.046036	3.821200
230.968113	4960.218775	7.349184	-0.046070	3.824147
231.051250	4968.270059	7.354189	-0.046090	3.827115
231.262201	4976.316119	7.359194	-0.046135	3.830082
231.591886	4984.331213	7.364198	-0.046201	3.833037
231.840227	4992.398028	7.369203	-0.046253	3.836008
231.945096	5000.348340	7.374208	-0.046278	3.838930
232.305132	5008.359365	7.379213	-0.046350	3.841877
232.488015	5016.385766	7.384218	-0.046389	3.844824
232.601089	5024.394179	7.389222	-0.046416	3.847761
233.005155	5032.453157	7.394227	-0.046496	3.850720
233.238920	5040.463070	7.399232	-0.046545	3.853656
233.369884	5048.517334	7.404237	-0.046574	3.856603
233.732214	5056.509530	7.409242	-0.046647	3.859530
233.786770	5064.515406	7.414246	-0.046663	3.862453
234.242791	5072.550843	7.419251	-0.046753	3.865393
234.150583	5080.609571	7.424256	-0.046741	3.868328
234.406125	5088.610087	7.429261	-0.046794	3.871247
234.853331	5096.903358	7.434266	-0.046882	3.874274
234.918435	5104.837368	7.439270	-0.046900	3.877160
235.122845	5112.753525	7.444275	-0.046943	3.880041
235.252363	5120.734711	7.449280	-0.046972	3.882941
235.406903	5128.730064	7.454285	-0.047006	3.885845
235.695464	5136.735562	7.459290	-0.047065	3.888753
236.006192	5144.762393	7.464294	-0.047128	3.891666
236.389183	5152.832127	7.469299	-0.047205	3.894595
236.794274	5160.815424	7.474304	-0.047285	3.897490
236.618747	5168.823943	7.479309	-0.047258	3.900381
237.096699	5176.851013	7.484314	-0.047352	3.903289
237.129068	5184.826045	7.489318	-0.047363	3.906168
237.357949	5192.853985	7.494323	-0.047411	3.909068
237.555709	5200.888725	7.499328	-0.047453	3.911967
237.773577	5208.934559	7.504333	-0.047499	3.914868
237.839192	5216.976879	7.509338	-0.047517	3.917763
237.927175	5224.968454	7.514342	-0.047538	3.920638
238.180144	5232.955838	7.519347	-0.047591	3.923513
238.477015	5240.974813	7.524352	-0.047651	3.926397
238.596205	5248.994828	7.529357	-0.047678	3.929276
238.907208	5257.055604	7.534362	-0.047742	3.932172
239.032991	5265.041035	7.539366	-0.047770	3.935035
239.399813	5273.074451	7.544371	-0.047844	3.937917
239.547212	5281.074143	7.549376	-0.047876	3.940781
239.726320	5289.071170	7.554381	-0.047915	3.943643
239.867294	5297.154658	7.559386	-0.047947	3.946532
239.996197	5305.131849	7.564390	-0.047976	3.949382
240.201296	5313.217981	7.569395	-0.048019	3.952269
240.538745	5321.237973	7.574400	-0.048087	3.955133
240.464815	5329.254004	7.579405	-0.048079	3.957987
240.705135	5337.262416	7.584410	-0.048129	3.960841
240.993796	5345.209406	7.589414	-0.048188	3.963672
241.285279	5353.233260	7.594419	-0.048247	3.966528
241.299152	5361.253369	7.599424	-0.048255	3.969377
241.587216	5369.311147	7.604429	-0.048314	3.972241
241.741434	5377.360928	7.609434	-0.048348	3.975098
241.753891	5385.358892	7.614438	-0.048355	3.977932
242.058692	5393.357712	7.619443	-0.048417	3.980769
242.308999	5401.371975	7.624448	-0.048469	3.983609
242.586818	5409.422592	7.629453	-0.048526	3.986460
242.831512	5417.461182	7.634458	-0.048577	3.989304
242.897213	5425.501472	7.639462	-0.048595	3.992144
243.121920	5433.539351	7.644467	-0.048642	3.994983
243.376725	5441.540928	7.649472	-0.048694	3.997808
243.877607	5449.498982	7.654477	-0.048793	4.000620
244.099591	5457.543776	7.659482	-0.048839	4.003456
244.165166	5465.582777	7.664486	-0.048857	4.006285
244.640518	5473.596683	7.669491	-0.048951	4.009110
244.691675	5481.622941	7.674496	-0.048965	4.011930
244.816943	5489.650692	7.679501	-0.048994	4.014750
245.121178	5497.691362	7.684506	-0.049056	4.017576
245.280007	5505.636434	7.689510	-0.049091	4.020363
245.522101	5513.661897	7.694515	-0.049141	4.023178
245.697869	5521.707584	7.699520	-0.049179	4.025998
245.842130	5529.735364	7.704525	-0.049211	4.028808
246.046774	5537.786752	7.709530	-0.049254	4.031626
246.215235	5545.876718	7.714534	-0.049291	4.034454
246.558168	5553.879066	7.719539	-0.049360	4.037253
246.615716	5561.793658	7.724544	-0.049376	4.040014
246.719360	5569.809392	7.729549	-0.049400	4.042810
247.009856	5577.830888	7.734554	-0.049460	4.045609
247.340330	5585.837544	7.739558	-0.049527	4.048401
247.378969	5593.892631	7.744563	-0.049539	4.051203
247.379442	5601.916280	7.749568	-0.049544	4.053993
247.852769	5609.924926	7.754573	-0.049638	4.056782
248.060861	5617.926860	7.759578	-0.049682	4.059562
248.033100	5625.933275	7.764582	-0.049682	4.062339
248.354128	5633.944396	7.769587	-0.049747	4.065121
248.604463	5641.950504	7.774592	-0.049799	4.067898
248.722918	5649.971151	7.779597	-0.049826	4.070676
248.973927	5658.054276	7.784602	-0.049878	4.073476
249.254227	5666.039814	7.789606	-0.049935	4.076241
249.479984	5674.009574	7.794611	-0.049983	4.078997
249.744055	5682.051148	7.799616	-0.050037	4.081777
249.847929	5690.015948	7.804621	-0.050061	4.084526
250.202845	5698.120310	7.809626	-0.050133	4.087325
250.197957	5706.111230	7.814630	-0.050137	4.090078
250.446258	5714.144834	7.819635	-0.050189	4.092847
250.913583	5722.176400	7.824640	-0.050281	4.095617
250.885030	5730.177339	7.829645	-0.050281	4.098367
251.157116	5738.226638	7.834650	-0.050337	4.101136
251.374381	5746.182629	7.839654	-0.050382	4.103871
251.664417	5754.283248	7.844659	-0.050442	4.106654
251.996646	5762.274953	7.849664	-0.050509	4.109399
252.193491	5770.309141	7.854669	-0.050551	4.112154
252.542377	5778.354973	7.859674	-0.050621	4.114914
252.390445	5786.373897	7.864678	-0.050598	4.117656
252.712509	5794.335802	7.869683	-0.050663	4.120383
252.849544	5802.347409	7.874688	-0.050694	4.123122
253.125685	5810.330960	7.879693	-0.050750	4.125852
253.285955	5818.425723	7.884698	-0.050785	4.128617
253.391768	5826.450122	7.889702	-0.050810	4.131355
253.768980	5834.471940	7.894707	-0.050886	4.134093
253.806122	5842.527946	7.899712	-0.050898	4.136837
253.789270	5850.493988	7.904717	-0.050900	4.139549
254.200760	5858.557479	7.909722	-0.050982	4.142296
254.288292	5866.498280	7.914726	-0.051004	4.144997
254.319102	5874.537311	7.919731	-0.051015	4.147728
254.654524	5882.567349	7.924736	-0.051082	4.150458
254.753924	5890.612853	7.929741	-0.051106	4.153188
254.929519	5898.655543	7.934746	-0.051144	4.155917
255.044880	5906.631920	7.939750	-0.051171	4.158620
255.329385	5914.658505	7.944755	-0.051229	4.161341
255.597087	5922.643040	7.949760	-0.051284	4.164046
255.773731	5930.647961	7.954765	-0.051322	4.166754
255.883352	5938.722344	7.959770	-0.051348	4.169484
256.094219	5946.709909	7.964774	-0.051392	4.172184
256.103093	5954.751083	7.969779	-0.051399	4.174897
256.408622	5962.759016	7.974784	-0.051461	4.177601
256.681736	5970.731631	7.979789	-0.051517	4.180291
256.809941	5978.795820	7.984794	-0.051546	4.183008
257.047814	5986.769903	7.989798	-0.051596	4.185695
257.393553	5994.801453	7.994803	-0.051665	4.188400
257.445312	6002.843100	7.999808	-0.051680	4.191104
257.465327	6010.949547	8.004813	-0.051689	4.193827
257.969731	6018.979000	8.009818	-0.051789	4.196528
258.216562	6026.893459	8.014822	-0.051840	4.199186
258.408253	6034.895801	8.019827	-0.051881	4.201871
258.580599	6042.901150	8.024832	-0.051918	4.204555
258.773573	6050.903595	8.029837	-0.051959	4.207236
258.855642	6058.900627	8.034842	-0.051980	4.209913
259.033527	6066.962447	8.039846	-0.052018	4.212611
259.429221	6074.995832	8.044851	-0.052097	4.215299
259.530274	6083.033077	8.049856	-0.052121	4.217985
259.749784	6090.976516	8.054861	-0.052167	4.220638
259.998912	6099.043083	8.059866	-0.052219	4.223331
259.953585	6107.030824	8.064870	-0.052215	4.225993
260.018580	6115.025988	8.069875	-0.052233	4.228657
260.173146	6123.118374	8.074880	-0.052267	4.231353
260.389412	6131.127850	8.079885	-0.052312	4.234019
260.628218	6139.209455	8.084890	-0.052362	4.236709
260.682040	6147.103250	8.089894	-0.052377	4.239332
260.977234	6155.182292	8.094899	-0.052437	4.242018
261.189130	6163.123055	8.099904	-0.052482	4.244655
261.110643	6171.221021	8.104909	-0.052473	4.247340
261.576310	6179.187468	8.109914	-0.052565	4.249984
261.870463	6187.249589	8.114918	-0.052625	4.252658
262.005121	6195.281639	8.119923	-0.052655	4.255317
262.172469	6203.315059	8.124928	-0.052691	4.257977
262.256769	6211.273627	8.129933	-0.052712	4.260608
262.500718	6219.345375	8.134938	-0.052763	4.263277
262.733950	6227.305289	8.139942	-0.052812	4.265908
262.985289	6235.376687	8.144947	-0.052864	4.268573
263.221527	6243.383556	8.149952	-0.052913	4.271216
263.367676	6251.463207	8.154957	-0.052945	4.273880
263.521955	6259.510778	8.159962	-0.052979	4.276531
263.920010	6267.408227	8.164966	-0.053059	4.279134
263.900730	6275.454142	8.169971	-0.053060	4.281781
264.179210	6283.435798	8.174976	-0.053117	4.284407
264.473332	6291.491473	8.179981	-0.053177	4.287056
264.664518	6299.495833	8.184986	-0.053218	4.289686
264.792192	6307.569566	8.189990	-0.053247	4.292336
265.296637	6315.564885	8.194995	-0.053346	4.294962
265.588783	6323.631428	8.200000	-0.053406	4.297608
265.681066	6331.577228	8.205005	-0.053429	4.300211
265.736013	6339.606057	8.210010	-0.053444	4.302839
266.188416	6347.612310	8.215014	-0.053533	4.305462
266.434410	6355.586432	8.220019	-0.053584	4.308071
266.676987	6363.645865	8.225024	-0.053635	4.310706
266.817574	6371.683032	8.230029	-0.053666	4.313331
267.005003	6379.720263	8.235034	-0.053706	4.315955
267.150996	6387.717440	8.240038	-0.053739	4.318564
267.227358	6395.705748	8.245043	-0.053758	4.321168
267.544564	6403.685890	8.250048	-0.053823	4.323770
267.644191	6411.718939	8.255053	-0.053846	4.326385
267.876570	6419.728079	8.260058	-0.053895	4.328992
268.070839	6427.757382	8.265062	-0.053936	4.331604
268.440106	6435.803242	8.270067	-0.054010	4.334221
268.743630	6443.852634	8.275072	-0.054072	4.336837
268.979707	6451.778524	8.280077	-0.054121	4.339411
269.215133	6459.852704	8.285082	-0.054170	4.342031
269.070029	6467.806769	8.290086	-0.054148	4.344608
269.219620	6475.853950	8.295091	-0.054182	4.347216
269.623522	6483.922097	8.300096	-0.054262	4.349831
269.736202	6491.968298	8.305101	-0.054288	4.352435
270.005348	6500.056825	8.310106	-0.054344	4.355052
270.205705	6508.000931	8.315110	-0.054386	4.357621
270.442364	6515.954906	8.320115	-0.054435	4.360191
270.364050	6523.958456	8.325120	-0.054426	4.362774
270.523720	6531.917645	8.330125	-0.054461	4.365342
270.860225	6540.035176	8.335130	-0.054529	4.367961
270.912252	6548.030257	8.340134	-0.054544	4.370538
271.138390	6556.025888	8.345139	-0.054591	4.373113
271.652678	6564.083160	8.350144	-0.054692	4.375709
271.702508	6572.054807	8.355149	-0.054707	4.378274
271.927885	6580.088244	8.360154	-0.054754	4.380857
272.093688	6588.046889	8.365158	-0.054790	4.383415
272.109778	6596.129610	8.370163	-0.054798	4.386010
272.357402	6604.124543	8.375168	-0.054850	4.388576
272.472555	6612.152831	8.380173	-0.054876	4.391151
272.761437	6620.193658	8.385178	-0.054935	4.393730
272.638817	6628.228679	8.390182	-0.054918	4.396302
272.904494	6636.200468	8.395187	-0.054972	4.398856
273.337117	6644.259197	8.400192	-0.055058	4.401436
273.584080	6652.173464	8.405197	-0.055109	4.403968
273.678306	6660.282480	8.410202	-0.055132	4.406559
273.817661	6668.267495	8.415206	-0.055163	4.409110
273.687685	6676.345548	8.420211	-0.055144	4.411687
274.058691	6684.358885	8.425216	-0.055219	4.414245
274.371470	6692.361257	8.430221	-0.055282	4.416798
274.566766	6700.351530	8.435226	-0.055324	4.419344
274.622223	6708.399568	8.440230	-0.055339	4.421907
274.863952	6716.372056	8.445235	-0.055390	4.424445
274.950497	6724.452602	8.450240	-0.055411	4.427016
275.033548	6732.416107	8.455245	-0.055432	4.429547
275.361499	6740.522332	8.460250	-0.055498	4.432124
275.409246	6748.520237	8.465254	-0.055512	4.434663
275.674145	6756.534554	8.470259	-0.055567	4.437208
276.055155	6764.511646	8.475264	-0.055643	4.439739
276.270660	6772.506481	8.480269	-0.055688	4.442274
276.645126	6780.474322	8.485274	-0.055763	4.444799
276.679290	6788.542971	8.490278	-0.055775	4.447353
276.827432	6796.539821	8.495283	-0.055808	4.449884
276.985463	6804.637953	8.500288	-0.055842	4.452445
277.173927	6812.604074	8.505293	-0.055883	4.454964
277.113360	6820.694467	8.510298	-0.055877	4.457519
277.164692	6828.625907	8.515302	-0.055891	4.460023
277.468230	6836.611345	8.520307	-0.055953	4.462543
277.437888	6844.651816	8.525312	-0.055953	4.465078
277.526381	6852.684608	8.530317	-0.055974	4.467610
277.874550	6860.703248	8.535322	-0.056044	4.470136
278.061171	6868.709484	8.540326	-0.056084	4.472657
278.245189	6876.733250	8.545331	-0.056124	4.475182
278.506581	6884.791606	8.550336	-0.056178	4.477716
278.652171	6892.761420	8.555341	-0.056210	4.480221
278.852771	6900.800831	8.560346	-0.056253	4.482746
279.099311	6908.745905	8.565351	-0.056304	4.485241
279.370828	6916.770923	8.570355	-0.056360	4.487759
279.726170	6924.805740	8.575360	-0.056431	4.490279
279.602714	6932.847704	8.580365	-0.056413	4.492799
279.872297	6940.893533	8.585370	-0.056469	4.495319
279.956800	6948.883789	8.590375	-0.056490	4.497820
280.381422	6956.885533	8.595379	-0.056574	4.500324
280.565702	6964.886978	8.600384	-0.056614	4.502826
280.854451	6972.876086	8.605389	-0.056673	4.505323
281.200386	6980.919281	8.610394	-0.056742	4.507836
281.422850	6988.954087	8.615399	-0.056789	4.510344
281.703956	6996.978987	8.620403	-0.056846	4.512848
282.092268	7005.062745	8.625408	-0.056924	4.515369
282.310573	7013.006104	8.630413	-0.056970	4.517844
282.530147	7021.021094	8.635418	-0.057016	4.520341
282.669973	7029.006049	8.640423	-0.057047	4.522826
283.042857	7037.006921	8.645427	-0.057122	4.525315
283.055895	7045.040854	8.650432	-0.057130	4.527813
283.373347	7053.048132	8.655437	-0.057194	4.530302
283.560686	7061.111038	8.660442	-0.057234	4.532806
283.695532	7069.104342	8.665447	-0.057264	4.535287
283.998672	7077.121237	8.670451	-0.057326	4.537774
284.094015	7085.105551	8.675456	-0.057349	4.540250
284.369742	7093.132592	8.680461	-0.057406	4.542737
284.642020	7101.157108	8.685466	-0.057462	4.545223
284.866699	7109.210588	8.690471	-0.057509	4.547716
284.973937	7117.187380	8.695475	-0.057534	4.550183
285.267758	7125.276773	8.700480	-0.057594	4.552685
285.166924	7133.240105	8.705485	-0.057580	4.555145
285.585061	7141.283355	8.710490	-0.057663	4.557629
285.584917	7149.191225	8.715495	-0.057668	4.560070
285.789555	7157.259452	8.720499	-0.057712	4.562559
285.846368	7165.294230	8.725504	-0.057728	4.565037
285.996269	7173.335103	8.730509	-0.057761	4.567515
286.241323	7181.345620	8.735514	-0.057812	4.569982
286.454428	7189.352553	8.740519	-0.057857	4.572447
286.557384	7197.355082	8.745523	-0.057881	4.574909
286.825442	7205.454961	8.750528	-0.057936	4.577400
286.893573	7213.347483	8.755533	-0.057954	4.579825
287.083028	7221.426953	8.760538	-0.057995	4.582307
287.066336	7229.392302	8.765543	-0.057997	4.584752
287.356032	7237.470219	8.770547	-0.058056	4.587230
287.792519	7245.517746	8.775552	-0.058142	4.589698
287.862304	7253.499023	8.780557	-0.058161	4.592144
288.020593	7261.560933	8.785562	-0.058195	4.594614
288.129763	7269.584466	8.790567	-0.058221	4.597070
288.346140	7277.494867	8.795571	-0.058266	4.599491
288.600245	7285.606579	8.800576	-0.058319	4.601972
288.766211	7293.496008	8.805581	-0.058355	4.604383
289.099583	7301.610386	8.810586	-0.058422	4.606862
289.087193	7309.566711	8.815591	-0.058425	4.609291
289.359657	7317.597849	8.820595	-0.058481	4.611742
289.427931	7325.658929	8.825600	-0.058499	4.614200
289.443346	7333.657733	8.830605	-0.058507	4.616639
289.786518	7341.651749	8.835610	-0.058576	4.619074
289.805354	7349.713453	8.840615	-0.058585	4.621529
290.093597	7357.675063	8.845619	-0.058644	4.623952
290.171298	7365.730037	8.850624	-0.058664	4.626402
290.368378	7373.667249	8.855629	-0.058706	4.628815
290.669905	7381.785619	8.860634	-0.058767	4.631282
290.628029	7389.767991	8.865639	-0.058765	4.633706
290.850515	7397.811638	8.870643	-0.058811	4.636148
291.043626	7405.752502	8.875648	-0.058852	4.638556
291.112260	7413.763197	8.880653	-0.058870	4.640985
291.461501	7421.827269	8.885658	-0.058941	4.643429
291.572108	7429.821878	8.890663	-0.058967	4.645850
291.632989	7437.824688	8.895667	-0.058983	4.648273
291.813422	7445.854785	8.900672	-0.059022	4.650703
292.159922	7453.901070	8.905677	-0.059092	4.653136
292.112923	7461.939992	8.910682	-0.059088	4.655565
292.221514	7469.926827	8.915687	-0.059114	4.657978
292.598372	7477.877531	8.920691	-0.059189	4.660378
292.848510	7485.955108	8.925696	-0.059241	4.662816
292.721587	7493.894589	8.930701	-0.059222	4.665211
292.962864	7501.966139	8.935706	-0.059273	4.667644
293.137309	7509.955666	8.940711	-0.059310	4.670051
293.450696	7518.046507	8.945715	-0.059374	4.672487
293.737622	7526.137417	8.950720	-0.059433	4.674922
293.706567	7534.074239	8.955725	-0.059432	4.677309
293.928850	7542.041424	8.960730	-0.059479	4.679704
294.009719	7550.074330	8.965735	-0.059499	4.682118
294.218441	7557.986371	8.970739	-0.059543	4.684495
294.386375	7566.121753	8.975744	-0.059580	4.686937
294.519324	7574.020820	8.980749	-0.059609	4.689306
294.759660	7582.144343	8.985754	-0.059659	4.691742
294.861689	7590.134791	8.990759	-0.059684	4.694137
294.937817	7598.130232	8.995763	-0.059703	4.696532
294.963094	7606.155507	9.000768	-0.059713	4.698935
295.160296	7614.147542	9.005773	-0.059755	4.701327
295.401143	7622.177462	9.010778	-0.059805	4.703728
295.643471	7630.188618	9.015783	-0.059855	4.706123
295.609166	7638.193435	9.020787	-0.059854	4.708515
295.898595	7646.235230	9.025792	-0.059913	4.710916
295.981884	7654.235621	9.030797	-0.059934	4.713304
296.261117	7662.301413	9.035802	-0.059991	4.715710
296.451308	7670.320410	9.040807	-0.060032	4.718101
296.747551	7678.234475	9.045811	-0.060092	4.720459
296.882152	7686.365013	9.050816	-0.060123	4.722881
297.150668	7694.341595	9.055821	-0.060178	4.725255
297.472413	7702.372117	9.060826	-0.060243	4.727644
297.660466	7710.403455	9.065831	-0.060283	4.730032
297.779107	7718.378380	9.070835	-0.060311	4.732403
298.066559	7726.446268	9.075840	-0.060369	4.734799
297.926060	7734.424640	9.080845	-0.060348	4.737169
298.113071	7742.424026	9.085850	-0.060389	4.739543
298.210459	7750.505499	9.090855	-0.060412	4.741940
298.516538	7758.431174	9.095859	-0.060474	4.744290
298.642076	7766.479039	9.100864	-0.060503	4.746675
298.465502	7774.517106	9.105869	-0.060475	4.749056
298.987463	7782.515377	9.110874	-0.060578	4.751423
299.216082	7790.573557	9.115879	-0.060625	4.753807
299.260580	7798.578823	9.120883	-0.060639	4.756174
299.525348	7806.563263	9.125888	-0.060693	4.758534
299.619999	7814.543376	9.130893	-0.060716	4.760892
299.675023	7822.550262	9.135898	-0.060732	4.763256
299.923699	7830.588964	9.140903	-0.060783	4.765629
300.217557	7838.600595	9.145907	-0.060843	4.767991
300.321963	7846.645649	9.150912	-0.060868	4.770363
300.534172	7854.653786	9.155917	-0.060913	4.772723
300.661318	7862.683927	9.160922	-0.060942	4.775088
300.617875	7870.664903	9.165927	-0.060939	4.777438
300.852107	7878.646167	9.170931	-0.060987	4.779786
301.103711	7886.731481	9.175936	-0.061040	4.782164
301.042660	7894.630663	9.180941	-0.061033	4.784487
301.324349	7902.795704	9.185946	-0.061091	4.786885
301.372543	7910.718121	9.190951	-0.061105	4.789212
301.535517	7918.743955	9.195955	-0.061141	4.791567
301.787307	7926.813438	9.200960	-0.061193	4.793934
301.678474	7934.831551	9.205965	-0.061178	4.796286
301.898263	7942.785066	9.210970	-0.061224	4.798617
302.015882	7950.834752	9.215975	-0.061251	4.800975
302.061516	7958.807353	9.220979	-0.061265	4.803310
302.371030	7966.859505	9.225984	-0.061328	4.805665
302.674432	7974.816372	9.230989	-0.061390	4.807992
302.792479	7982.901294	9.235994	-0.061417	4.810355
302.895723	7990.477168	9.240999	-0.061441	4.812569
303.289937	7995.070905	9.246003	-0.061517	4.813909
303.465740	7997.522385	9.251008	-0.061552	4.814625
303.343047	7998.834035	9.256013	-0.061530	4.815008
303.640460	7999.594735	9.261018	-0.061586	4.815229
303.556906	7999.604038	9.266023	-0.061570	4.815232
303.659426	8000.216153	9.271027	-0.061590	4.815410
303.876765	8000.007027	9.276032	-0.061630	4.815348
303.976953	8000.229985	9.281037	-0.061649	4.815413
303.765462	8000.047941	9.286042	-0.061609	4.815361
304.012905	8000.197443	9.291047	-0.061655	4.815403
304.074980	8000.298967	9.296051	-0.061667	4.815433
304.252138	8000.005786	9.301056	-0.061700	4.815346
304.190047	8000.222841	9.306061	-0.061689	4.815410
304.444586	8000.029298	9.311066	-0.061736	4.815352
304.601201	8000.073595	9.316071	-0.061765	4.815364
304.316423	8000.126591	9.321075	-0.061712	4.815381
304.453589	8000.083972	9.326080	-0.061738	4.815368
304.507027	8000.460103	9.331085	-0.061748	4.815478
304.543170	8000.088670	9.336090	-0.061754	4.815369
304.623519	8000.051521	9.341095	-0.061769	4.815358
304.652537	8000.061625	9.346099	-0.061775	4.815360
304.872512	8000.072766	9.351104	-0.061816	4.815363
304.676174	7999.940148	9.356109	-0.061779	4.815325
304.751489	7999.963851	9.361114	-0.061793	4.815331
304.826730	8000.210986	9.366119	-0.061807	4.815403
304.857713	8000.108872	9.371123	-0.061813	4.815373
305.021903	8000.017525	9.376128	-0.061843	4.815346
305.051250	8000.180512	9.381133	-0.061849	4.815393
305.047721	8000.058580	9.386138	-0.061848	4.815358
305.169689	8000.046711	9.391143	-0.061871	4.815354
305.093531	8000.053999	9.396147	-0.061857	4.815356
305.200948	7999.872976	9.401152	-0.061877	4.815303
304.945754	8000.103928	9.406157	-0.061829	4.815371
304.934785	8000.198893	9.411162	-0.061827	4.815399
304.979607	7999.982619	9.416167	-0.061836	4.815336
304.972305	8000.302150	9.421171	-0.061834	4.815429
305.017255	8000.057012	9.426176	-0.061843	4.815357
305.255716	8000.197819	9.431181	-0.061887	4.815397
305.229658	8000.060545	9.436186	-0.061882	4.815357
305.161751	8000.090420	9.441191	-0.061870	4.815366
304.974594	8000.081964	9.446195	-0.061835	4.815365
305.221303	8000.104241	9.451200	-0.061881	4.815370
305.322097	8000.026806	9.456205	-0.061899	4.815347
305.544691	8000.000574	9.461210	-0.061941	4.815338
305.735486	7999.995195	9.466215	-0.061976	4.815336
305.705752	7999.994702	9.471219	-0.061971	4.815336
305.588599	7999.977787	9.476224	-0.061949	4.815331
305.654413	8000.156350	9.481229	-0.061961	4.815383
305.557522	7999.994378	9.486234	-0.061943	4.815336
305.522639	7999.960657	9.491239	-0.061937	4.815327
305.705264	7999.998974	9.496243	-0.061971	4.815337
305.762308	7999.808560	9.501248	-0.061981	4.815281
305.572262	8000.116501	9.506253	-0.061946	4.815372
305.594192	7999.868841	9.511258	-0.061950	4.815300
305.774953	7999.983031	9.516263	-0.061984	4.815332
305.675251	8000.070108	9.521267	-0.061965	4.815358
305.703177	7999.793683	9.526272	-0.061970	4.815277
305.805733	8000.080832	9.531277	-0.061990	4.815360
306.015318	7999.894022	9.536282	-0.062029	4.815305
305.870948	8000.026326	9.541287	-0.062002	4.815344
305.810721	8000.077711	9.546291	-0.061991	4.815360
306.013783	8000.047947	9.551296	-0.062028	4.815350
305.968818	8000.170146	9.556301	-0.062020	4.815386
305.965457	8000.007589	9.561306	-0.062019	4.815338
306.221669	8000.047131	9.566311	-0.062067	4.815349
306.164346	8000.077182	9.571315	-0.062057	4.815358
306.199333	8000.013619	9.576320	-0.062063	4.815339
306.158833	8000.035398	9.581325	-0.062056	4.815345
306.311155	7999.996237	9.586330	-0.062084	4.815333
306.159573	7999.995855	9.591335	-0.062056	4.815334
305.947292	8000.204006	9.596339	-0.062016	4.815396
306.029262	8000.010795	9.601344	-0.062031	4.815339
306.096883	8000.017266	9.606349	-0.062044	4.815340
306.072152	8000.001889	9.611354	-0.062039	4.815336
306.288736	8000.023666	9.616359	-0.062080	4.815341
306.359377	8000.140305	9.621363	-0.062093	4.815375
306.396846	7999.899313	9.626368	-0.062100	4.815305
306.203928	7999.964527	9.631373	-0.062064	4.815325
306.112894	7999.963014	9.636378	-0.062047	4.815325
306.075915	7999.974160	9.641383	-0.062040	4.815328
306.104907	7999.939363	9.646387	-0.062046	4.815318
306.583010	7999.876756	9.651392	-0.062135	4.815297
306.561086	7999.890290	9.656397	-0.062130	4.815301
306.370613	8000.028243	9.661402	-0.062095	4.815342
306.383722	7999.935451	9.666407	-0.062097	4.815315
306.354452	8000.034391	9.671411	-0.062092	4.815344
306.396962	7999.865113	9.676416	-0.062100	4.815295
306.417844	8000.141288	9.681421	-0.062104	4.815375
306.455612	8000.046767	9.686426	-0.062111	4.815347
306.448202	7999.865968	9.691431	-0.062110	4.815295
306.492601	8000.159640	9.696435	-0.062118	4.815380
306.733772	7999.915621	9.701440	-0.062163	4.815308
306.686322	7999.946906	9.706445	-0.062154	4.815317
306.492955	7999.811123	9.711450	-0.062118	4.815278
306.724696	7999.978550	9.716455	-0.062161	4.815326
306.625660	7999.927725	9.721459	-0.062143	4.815312
306.584194	7999.911000	9.726464	-0.062135	4.815307
306.501715	8000.025091	9.731469	-0.062120	4.815341
306.580204	7999.898106	9.736474	-0.062134	4.815303
306.642559	7999.964359	9.741479	-0.062146	4.815322
306.422244	7999.953211	9.746483	-0.062105	4.815320
306.492657	7999.865649	9.751488	-0.062118	4.815294
306.516600	7999.963335	9.756493	-0.062122	4.815323
306.591175	8000.123873	9.761498	-0.062136	4.815369
306.498561	8000.072085	9.766503	-0.062119	4.815355
306.607731	8000.124150	9.771507	-0.062140	4.815369
306.937061	7999.939329	9.776512	-0.062201	4.815314
306.722573	8000.142099	9.781517	-0.062161	4.815374
306.593385	7999.986000	9.786522	-0.062137	4.815329
306.591779	8000.010563	9.791527	-0.062137	4.815336
306.485435	8000.176644	9.796531	-0.062117	4.815385
306.814133	7999.947980	9.801536	-0.062178	4.815317
306.975677	7999.849103	9.806541	-0.062208	4.815287
306.737214	7999.917836	9.811546	-0.062164	4.815308
306.816972	7999.869985	9.816551	-0.062178	4.815294
306.834584	8000.010331	9.821555	-0.062182	4.815335
306.728640	7999.987188	9.826560	-0.062162	4.815329
306.558068	8000.067741	9.831565	-0.062130	4.815353
306.933913	7999.954255	9.836570	-0.062200	4.815318
307.029700	7999.922707	9.841575	-0.062218	4.815308
306.736325	8000.066433	9.846579	-0.062164	4.815352
306.790911	7999.815034	9.851584	-0.062174	4.815278
306.889557	7999.969557	9.856589	-0.062192	4.815323
306.751559	8000.002543	9.861594	-0.062166	4.815333
306.662153	7999.955085	9.866599	-0.062150	4.815320
306.898496	7999.960086	9.871603	-0.062194	4.815320
306.964673	7999.810445	9.876608	-0.062206	4.815276
306.829733	7999.942908	9.881613	-0.062181	4.815315
306.886991	7999.945999	9.886618	-0.062192	4.815316
307.158408	7999.810463	9.891623	-0.062242	4.815275
306.808437	7999.978906	9.896627	-0.062177	4.815326
306.957336	7999.885164	9.901632	-0.062205	4.815298
306.781877	8000.052234	9.906637	-0.062172	4.815347
306.826299	8000.010209	9.911642	-0.062180	4.815335
306.845976	7999.829859	9.916647	-0.062184	4.815282
306.914110	8000.071542	9.921651	-0.062197	4.815352
307.143350	7999.830531	9.926656	-0.062239	4.815281
306.791130	8000.020319	9.931661	-0.062174	4.815338
306.833003	7999.800782	9.936666	-0.062182	4.815274
306.872923	7999.944706	9.941671	-0.062189	4.815316
307.009213	7999.920246	9.946675	-0.062214	4.815308
307.010440	7999.958755	9.951680	-0.062215	4.815319
306.993214	7999.962746	9.956685	-0.062212	4.815320
307.076486	7999.891433	9.961690	-0.062227	4.815299
307.042265	7999.855584	9.966695	-0.062221	4.815289
307.102820	7999.942121	9.971699	-0.062232	4.815314
307.160367	7999.810510	9.976704	-0.062243	4.815275
306.916612	7999.946509	9.981709	-0.062197	4.815316
307.041586	7999.936828	9.986714	-0.062221	4.815312
306.931001	7999.974547	9.991719	-0.062200	4.815324
306.898491	8000.018909	9.996723	-0.062194	4.815337
306.919223	7999.941210	10.001728	-0.062198	4.815314
306.860699	7999.887851	10.006733	-0.062187	4.815299
306.874561	7999.834628	10.011738	-0.062189	4.815283
307.144264	7999.941749	10.016743	-0.062240	4.815313
307.080762	7999.948177	10.021747	-0.062228	4.815316
307.105009	7999.876952	10.026752	-0.062232	4.815295
307.063981	7999.967144	10.031757	-0.062225	4.815321
307.154760	7999.966517	10.036762	-0.062242	4.815321
307.250744	7999.953147	10.041767	-0.062260	4.815316
306.972317	7999.950654	10.046771	-0.062208	4.815317
307.103102	7999.949624	10.051776	-0.062232	4.815316
307.015582	7999.977034	10.056781	-0.062216	4.815324
307.064671	7999.836730	10.061786	-0.062225	4.815283
307.139066	7999.928842	10.066791	-0.062239	4.815310
306.943319	8000.016461	10.071795	-0.062203	4.815336
307.107472	8000.092962	10.076800	-0.062233	4.815358
307.057132	7999.924275	10.081805	-0.062224	4.815309
307.021250	7999.824252	10.086810	-0.062217	4.815280
307.093085	7999.944118	10.091815	-0.062230	4.815314
307.156350	7999.945172	10.096819	-0.062242	4.815314
307.186124	7999.829135	10.101824	-0.062248	4.815280
307.301423	7999.918721	10.106829	-0.062269	4.815306
307.232896	7999.991351	10.111834	-0.062257	4.815327
307.075422	8000.094574	10.116839	-0.062227	4.815358
307.083333	7999.945030	10.121843	-0.062229	4.815315
307.382463	7999.878378	10.126848	-0.062284	4.815294
307.274416	8000.089335	10.131853	-0.062264	4.815356
307.188101	7999.959606	10.136858	-0.062248	4.815318
307.193153	7999.841019	10.141863	-0.062249	4.815284
307.338982	7999.957841	10.146867	-0.062276	4.815317
307.367132	7999.954034	10.151872	-0.062282	4.815316
307.301734	7999.986089	10.156877	-0.062269	4.815326
307.274691	8000.070101	10.161882	-0.062264	4.815350
307.206792	7999.933194	10.166887	-0.062252	4.815311
307.051587	8000.159403	10.171891	-0.062223	4.815377
307.209893	7999.870170	10.176896	-0.062252	4.815292
307.319482	8000.027016	10.181901	-0.062273	4.815337
307.368855	7999.932687	10.186906	-0.062282	4.815310
307.310421	7999.883605	10.191911	-0.062271	4.815296
307.268880	7999.970582	10.196915	-0.062263	4.815321
307.337328	7999.815632	10.201920	-0.062276	4.815276
307.307007	7999.968011	10.206925	-0.062270	4.815320
307.400476	7999.932148	10.211930	-0.062288	4.815309
307.383646	7999.957528	10.216935	-0.062285	4.815317
307.410262	7999.928036	10.221939	-0.062290	4.815308
307.510884	7999.922227	10.226944	-0.062308	4.815306
307.428524	7999.957208	10.231949	-0.062293	4.815316
307.269172	8000.065746	10.236954	-0.062264	4.815349
307.464555	7999.954602	10.241959	-0.062300	4.815316
307.507046	7999.985245	10.246963	-0.062308	4.815324
307.258438	7999.876336	10.251968	-0.062261	4.815294
307.237952	7999.995737	10.256973	-0.062258	4.815329
307.369212	7999.978678	10.261978	-0.062282	4.815323
307.376360	7999.919996	10.266983	-0.062283	4.815306
307.242015	8000.121963	10.271987	-0.062259	4.815365
307.510970	8000.158514	10.276992	-0.062309	4.815375
307.424273	7999.868409	10.281997	-0.062292	4.815291
307.301237	7999.900575	10.287002	-0.062270	4.815301
307.245988	8000.079268	10.292007	-0.062259	4.815353
307.340083	8000.029517	10.297011	-0.062277	4.815338
307.470883	7999.896985	10.302016	-0.062301	4.815299
307.312036	8000.100683	10.307021	-0.062272	4.815359
307.408190	7999.994303	10.312026	-0.062290	4.815327
307.429203	7999.888811	10.317031	-0.062293	4.815296
307.109111	8000.158249	10.322035	-0.062234	4.815377
307.299618	7999.973255	10.327040	-0.062269	4.815322
307.370940	8000.157262	10.332045	-0.062283	4.815375
307.285661	7999.993337	10.337050	-0.062267	4.815328
307.259524	7999.923411	10.342055	-0.062262	4.815307
307.366770	7999.978652	10.347059	-0.062282	4.815323
307.457942	7999.933129	10.352064	-0.062299	4.815309
307.496402	8000.029991	10.357069	-0.062306	4.815337
307.384283	8000.049508	10.362074	-0.062285	4.815344
307.487150	8000.000972	10.367079	-0.062304	4.815329
307.305045	8000.150827	10.372083	-0.062271	4.815374
307.529027	7999.937523	10.377088	-0.062312	4.815310
307.412073	8000.118398	10.382093	-0.062290	4.815364
307.497496	8000.083470	10.387098	-0.062306	4.815353
307.481759	7999.923910	10.392103	-0.062303	4.815306
307.398333	8000.016605	10.397107	-0.062288	4.815334
307.548770	7999.969930	10.402112	-0.062316	4.815320
307.472933	7999.952632	10.407117	-0.062302	4.815315
307.562010	8000.004364	10.412122	-0.062318	4.815330
307.426658	7999.940103	10.417127	-0.062293	4.815311
307.517306	7999.946958	10.422131	-0.062310	4.815313
307.543431	7999.810547	10.427136	-0.062315	4.815273
307.475323	8000.137635	10.432141	-0.062302	4.815369
307.481999	8000.146300	10.437146	-0.062304	4.815371
307.467987	7999.987837	10.442151	-0.062301	4.815325
307.655773	7999.988824	10.447155	-0.062336	4.815325
307.804941	7999.915400	10.452160	-0.062364	4.815302
307.769762	8000.026005	10.457165	-0.062357	4.815335
307.665689	7999.924845	10.462170	-0.062338	4.815306
307.840702	7999.907445	10.467175	-0.062370	4.815300
307.664764	7999.949421	10.472179	-0.062338	4.815313
307.758806	7999.937088	10.477184	-0.062355	4.815309
307.786070	8000.111811	10.482189	-0.062360	4.815360
307.665811	8000.001828	10.487194	-0.062338	4.815328
307.656713	7999.996332	10.492199	-0.062336	4.815327
307.622013	8000.022483	10.497203	-0.062330	4.815335
307.841639	7999.953439	10.502208	-0.062371	4.815313
307.893587	8000.029143	10.507213	-0.062380	4.815335
307.740751	8000.042637	10.512218	-0.062352	4.815340
307.744332	7999.880191	10.517223	-0.062352	4.815292
307.615379	7999.956092	10.522227	-0.062329	4.815315
307.608220	7999.920692	10.527232	-0.062327	4.815305
307.752167	7999.991513	10.532237	-0.062354	4.815325
307.757185	8000.024740	10.537242	-0.062355	4.815335
307.754397	7999.997966	10.542247	-0.062354	4.815327
307.980699	8000.027393	10.547251	-0.062397	4.815334
307.826381	7999.917912	10.552256	-0.062368	4.815303
307.802534	8000.054365	10.557261	-0.062363	4.815343
307.782108	8000.119243	10.562266	-0.062360	4.815362
308.102120	7999.789932	10.567271	-0.062419	4.815264
308.080317	8000.053646	10.572275	-0.062415	4.815341
307.678012	7999.852370	10.577280	-0.062340	4.815285
307.874128	7999.868463	10.582285	-0.062377	4.815288
307.908348	7999.971670	10.587290	-0.062383	4.815318
307.850621	7999.960019	10.592295	-0.062372	4.815315
307.805798	7999.944306	10.597299	-0.062364	4.815311
307.796891	7999.944159	10.602304	-0.062362	4.815311
307.757382	7999.937087	10.607309	-0.062355	4.815309
307.607345	8000.153763	10.612314	-0.062327	4.815373
307.913394	7999.906542	10.617319	-0.062384	4.815299
307.777822	7999.965227	10.622323	-0.062359	4.815317
307.771194	7999.920215	10.627328	-0.062358	4.815304
307.582307	7999.979081	10.632333	-0.062323	4.815322
307.674830	8000.026594	10.637338	-0.062340	4.815335
307.866489	7999.871554	10.642343	-0.062375	4.815289
307.837156	8000.070994	10.647347	-0.062370	4.815348
308.050832	7999.875693	10.652352	-0.062410	4.815290
307.875522	7999.947615	10.657357	-0.062377	4.815311
307.861499	8000.151587	10.662362	-0.062375	4.815371
307.926227	7999.921732	10.667367	-0.062387	4.815304
308.037571	7999.936416	10.672371	-0.062407	4.815307
307.825795	7999.843086	10.677376	-0.062368	4.815281
307.894771	7999.934041	10.682381	-0.062381	4.815307
308.011425	7999.965919	10.687386	-0.062403	4.815316
308.142978	7999.790634	10.692391	-0.062427	4.815264
308.013730	8000.063251	10.697395	-0.062403	4.815345
307.898853	7999.950150	10.702400	-0.062382	4.815312
308.042639	8000.111845	10.707405	-0.062409	4.815359
307.927013	7999.958104	10.712410	-0.062387	4.815314
307.903765	7999.938473	10.717415	-0.062383	4.815309
308.125311	7999.934678	10.722419	-0.062424	4.815306
308.139184	7999.908181	10.727424	-0.062426	4.815299
308.144969	7999.931799	10.732429	-0.062428	4.815306
308.108660	7999.946164	10.737434	-0.062421	4.815310
308.029557	7999.814414	10.742439	-0.062406	4.815272
308.055199	8000.122753	10.747443	-0.062411	4.815362
307.951209	7999.803490	10.752448	-0.062391	4.815269
307.933780	7999.955017	10.757453	-0.062388	4.815313
307.879444	8000.112345	10.762458	-0.062378	4.815360
308.026314	7999.902033	10.767463	-0.062405	4.815297
307.924472	7999.949519	10.772467	-0.062387	4.815312
307.901949	7999.924555	10.777472	-0.062382	4.815305
308.012747	8000.057904	10.782477	-0.062403	4.815343
308.061480	7999.936834	10.787482	-0.062412	4.815307
308.141544	7999.898610	10.792487	-0.062427	4.815296
308.247443	8000.174074	10.797491	-0.062447	4.815376
308.314480	7999.965638	10.802496	-0.062459	4.815315
308.176591	7999.952652	10.807501	-0.062434	4.815311
308.130544	8000.024588	10.812506	-0.062425	4.815333
308.321470	7999.847083	10.817511	-0.062461	4.815280
308.234597	7999.854191	10.822515	-0.062444	4.815282
308.079691	7999.830231	10.827520	-0.062415	4.815276
308.109705	7999.862805	10.832525	-0.062421	4.815286
307.862470	7999.997679	10.837530	-0.062375	4.815326
307.996414	7999.812811	10.842535	-0.062400	4.815271
308.016282	7999.892258	10.847539	-0.062404	4.815295
308.137191	7999.883580	10.852544	-0.062426	4.815291
307.997899	7999.919751	10.857549	-0.062400	4.815303
307.936456	8000.101552	10.862554	-0.062389	4.815356
308.114365	7999.937728	10.867559	-0.062422	4.815307
308.185538	8000.112115	10.872563	-0.062435	4.815358
308.349383	7999.804793	10.877568	-0.062466	4.815267
308.340031	7999.991737	10.882573	-0.062464	4.815322
308.240730	8000.084169	10.887578	-0.062446	4.815350
308.110688	7999.977230	10.892583	-0.062421	4.815319
307.968263	7999.987689	10.897587	-0.062395	4.815323
308.038781	7999.945030	10.902592	-0.062408	4.815310
308.242592	7999.955907	10.907597	-0.062446	4.815312
308.074741	8000.119900	10.912602	-0.062415	4.815361
308.051942	7999.971980	10.917607	-0.062411	4.815318
308.059355	7999.957136	10.922611	-0.062412	4.815313
308.052136	7999.976261	10.927616	-0.062411	4.815319
308.200821	8000.010811	10.932621	-0.062438	4.815328
308.208781	8000.154210	10.937626	-0.062440	4.815370
308.192763	7999.962567	10.942631	-0.062437	4.815314
308.018524	8000.028093	10.947635	-0.062404	4.815334
308.110040	8000.108734	10.952640	-0.062422	4.815357
308.246645	7999.979504	10.957645	-0.062447	4.815319
307.974553	8000.097927	10.962650	-0.062396	4.815355
308.178806	7999.922781	10.967655	-0.062434	4.815303
308.180025	8000.015818	10.972659	-0.062435	4.815330
308.110708	8000.014665	10.977664	-0.062422	4.815330
308.093463	8000.256006	10.982669	-0.062419	4.815400
308.093814	8000.110608	10.987674	-0.062419	4.815358
308.065798	7999.888831	10.992679	-0.062413	4.815293
308.035391	7999.931091	10.997683	-0.062408	4.815306
308.057179	7999.993464	11.002688	-0.062412	4.815324
308.157647	7999.874325	11.007693	-0.062430	4.815289
308.070580	8000.109156	11.012698	-0.062414	4.815358
308.264170	7999.814090	11.017703	-0.062450	4.815271
308.206413	8000.065446	11.022707	-0.062440	4.815344
308.079145	7999.839879	11.027712	-0.062416	4.815279
308.057135	7999.825615	11.032717	-0.062412	4.815275
308.247357	8000.111035	11.037722	-0.062447	4.815357
308.284687	7999.932041	11.042727	-0.062454	4.815305
308.078357	8000.019484	11.047731	-0.062416	4.815331
308.189836	8000.078005	11.052736	-0.062437	4.815348
308.160356	7999.870103	11.057741	-0.062431	4.815287
308.116555	7999.929246	11.062746	-0.062423	4.815305
308.086544	7999.820765	11.067751	-0.062417	4.815273
308.091121	8000.047499	11.072755	-0.062418	4.815340
308.153420	7999.837917	11.077760	-0.062430	4.815278
308.229881	7999.841328	11.082765	-0.062444	4.815279
308.140403	7999.926440	11.087770	-0.062427	4.815304
308.250051	7999.811730	11.092775	-0.062448	4.815270
308.346452	8000.083828	11.097779	-0.062466	4.815349
308.116937	7999.901462	11.102784	-0.062423	4.815297
308.310786	7999.936763	11.107789	-0.062459	4.815306
308.165449	8000.030568	11.112794	-0.062432	4.815334
308.175572	7999.952690	11.117799	-0.062434	4.815311
308.094586	8000.074294	11.122803	-0.062419	4.815347
308.336173	7999.913668	11.127808	-0.062464	4.815299
308.204844	7999.927520	11.132813	-0.062439	4.815304
308.427591	8000.029590	11.137818	-0.062481	4.815333
308.496743	7999.838297	11.142823	-0.062494	4.815276
308.179488	7999.970936	11.147827	-0.062435	4.815317
308.153400	8000.036789	11.152832	-0.062430	4.815336
308.266221	7999.921062	11.157837	-0.062451	4.815302
308.241862	8000.121657	11.162842	-0.062447	4.815360
308.232872	7999.823218	11.167847	-0.062445	4.815273
308.245686	7999.957074	11.172851	-0.062447	4.815312
308.243982	7999.829819	11.177856	-0.062447	4.815275
308.256957	7999.955125	11.182861	-0.062449	4.815312
308.218646	8000.025051	11.187866	-0.062442	4.815332
308.314544	7999.834204	11.192871	-0.062460	4.815276
308.534073	7999.882762	11.197875	-0.062501	4.815289
308.512292	7999.803284	11.202880	-0.062497	4.815266
308.322159	7999.903827	11.207885	-0.062461	4.815296
308.289779	7999.910773	11.212890	-0.062455	4.815299
308.328086	7999.939209	11.217895	-0.062463	4.815307
308.291994	7999.951439	11.222899	-0.062456	4.815311
308.361116	8000.180319	11.227904	-0.062469	4.815377
308.395168	7999.905046	11.232909	-0.062475	4.815296
308.183003	8000.177355	11.237914	-0.062436	4.815377
308.366848	7999.949481	11.242919	-0.062470	4.815310
308.245455	7999.961360	11.247923	-0.062447	4.815314
308.194001	7999.834346	11.252928	-0.062438	4.815277
308.371196	7999.852264	11.257933	-0.062471	4.815281
308.257078	7999.821499	11.262938	-0.062449	4.815273
308.401538	7999.932956	11.267943	-0.062476	4.815305
308.255895	7999.889906	11.272947	-0.062449	4.815293
308.330237	7999.839826	11.277952	-0.062463	4.815278
308.335353	7999.942549	11.282957	-0.062464	4.815308
308.141073	7999.835610	11.287962	-0.062428	4.815277
308.368835	7999.814811	11.292967	-0.062470	4.815270
308.353805	7999.939651	11.297971	-0.062468	4.815307
308.133542	7999.928502	11.302976	-0.062427	4.815305
308.302635	7999.866100	11.307981	-0.062458	4.815286
308.127322	7999.939091	11.312986	-0.062425	4.815308
308.155341	7999.837991	11.317991	-0.062431	4.815278
308.098343	7999.932196	11.322995	-0.062420	4.815306
308.293719	7999.935449	11.328000	-0.062456	4.815306
308.255374	7999.857834	11.333005	-0.062449	4.815283
308.219723	8000.110627	11.338010	-0.062443	4.815357
308.341396	7999.943729	11.343015	-0.062465	4.815308
308.248539	8000.133561	11.348019	-0.062448	4.815364
308.340800	7999.986486	11.353024	-0.062465	4.815321
308.540158	8000.004774	11.358029	-0.062502	4.815325
308.550277	7999.920481	11.363034	-0.062504	4.815300
308.614249	7999.943999	11.368039	-0.062516	4.815307
308.401710	7999.874175	11.373043	-0.062477	4.815287
308.437771	7999.945339	11.378048	-0.062483	4.815308
308.401810	7999.927635	11.383053	-0.062477	4.815303
308.375231	8000.118571	11.388058	-0.062472	4.815359
308.418239	8000.098974	11.393063	-0.062480	4.815353
308.388015	7999.969105	11.398067	-0.062474	4.815315
308.345486	7999.934185	11.403072	-0.062466	4.815305
308.345612	7999.852934	11.408077	-0.062466	4.815281
308.270075	7999.832433	11.413082	-0.062452	4.815276
308.485723	7999.829608	11.418087	-0.062492	4.815274
308.225245	7999.931118	11.423091	-0.062444	4.815305
308.146523	7999.937293	11.428096	-0.062429	4.815307
308.393614	7999.820594	11.433101	-0.062475	4.815272
308.479521	8000.044406	11.438106	-0.062491	4.815337
308.501593	7999.980626	11.443111	-0.062495	4.815318
308.220628	8000.186571	11.448115	-0.062443	4.815380
308.297661	7999.839314	11.453120	-0.062457	4.815278
308.338558	7999.943702	11.458125	-0.062465	4.815308
308.291433	8000.046625	11.463130	-0.062456	4.815338
308.316238	7999.875976	11.468135	-0.062461	4.815288
308.303876	7999.942058	11.473139	-0.062459	4.815308
308.395190	7999.863394	11.478144	-0.062476	4.815284
308.407139	7999.892460	11.483149	-0.062478	4.815293
308.321479	7999.807643	11.488154	-0.062462	4.815268
308.401615	7999.928721	11.493159	-0.062477	4.815303
308.372319	7999.967792	11.498163	-0.062471	4.815315
308.322515	8000.132682	11.503168	-0.062462	4.815363
308.297893	7999.914167	11.508173	-0.062458	4.815300
308.251891	8000.093018	11.513178	-0.062449	4.815352
308.361371	7999.921640	11.518183	-0.062469	4.815301
308.457105	8000.009835	11.523187	-0.062487	4.815327
308.663569	7999.891391	11.528192	-0.062526	4.815291
308.768438	7999.944456	11.533197	-0.062545	4.815306
308.489236	7999.931256	11.538202	-0.062493	4.815304
308.603454	7999.820898	11.543207	-0.062514	4.815271
308.735758	7999.842346	11.548211	-0.062539	4.815276
308.539959	7999.825189	11.553216	-0.062503	4.815272
308.484983	7999.851003	11.558221	-0.062492	4.815280
308.540793	7999.818790	11.563226	-0.062503	4.815271
308.642193	7999.837585	11.568231	-0.062522	4.815276
308.470226	7999.860383	11.573235	-0.062490	4.815283
308.467733	7999.958703	11.578240	-0.062489	4.815312
308.648902	7999.903986	11.583245	-0.062523	4.815295
308.478832	7999.953544	11.588250	-0.062491	4.815310
308.648318	7999.808824	11.593255	-0.062523	4.815267
308.589633	7999.846337	11.598259	-0.062512	4.815278
308.371499	7999.930377	11.603264	-0.062471	4.815304
308.445916	7999.806527	11.608269	-0.062485	4.815267
308.466413	7999.960825	11.613274	-0.062489	4.815312
308.651527	7999.856993	11.618279	-0.062524	4.815281
308.652717	7999.943615	11.623283	-0.062524	4.815306
308.563232	7999.873701	11.628288	-0.062507	4.815286
308.674583	7999.841343	11.633293	-0.062528	4.815276
308.538471	8000.031524	11.638298	-0.062503	4.815333
308.502057	7999.731559	11.643303	-0.062496	4.815245
308.640428	7999.943415	11.648307	-0.062522	4.815306
308.542557	7999.896882	11.653312	-0.062503	4.815293
308.430524	7999.824455	11.658317	-0.062482	4.815273
308.577110	8000.024688	11.663322	-0.062510	4.815331
308.601824	7999.804856	11.668327	-0.062514	4.815266
308.353459	7999.955748	11.673331	-0.062468	4.815311
308.411335	7999.842315	11.678336	-0.062479	4.815278
308.757088	7999.898320	11.683341	-0.062543	4.815293
308.608346	8000.149234	11.688346	-0.062516	4.815367
308.521368	7999.954270	11.693351	-0.062500	4.815310
308.484681	7999.964352	11.698355	-0.062493	4.815313
308.475223	7999.874387	11.703360	-0.062491	4.815287
308.751079	7999.833007	11.708365	-0.062542	4.815274
308.701713	7999.955138	11.713370	-0.062533	4.815310
308.592606	7999.937285	11.718375	-0.062513	4.815305
308.624364	7999.898256	11.723379	-0.062519	4.815293
308.609970	7999.998517	11.728384	-0.062516	4.815323
308.691397	7999.855539	11.733389	-0.062531	4.815281
308.482451	7999.956838	11.738394	-0.062492	4.815311
308.409051	7999.932096	11.743399	-0.062479	4.815304
308.473169	7999.943855	11.748403	-0.062491	4.815307
308.453521	7999.958497	11.753408	-0.062487	4.815312
308.534858	7999.833693	11.758413	-0.062502	4.815275
308.325800	7999.944612	11.763418	-0.062463	4.815308
308.431122	7999.800964	11.768423	-0.062483	4.815266
308.451821	7999.860111	11.773427	-0.062487	4.815283
308.464282	7999.929814	11.778432	-0.062489	4.815303
308.744274	7999.859635	11.783437	-0.062541	4.815281
308.749135	7999.930281	11.788442	-0.062542	4.815302
308.636563	7999.832185	11.793447	-0.062521	4.815274
308.606515	8000.033754	11.798451	-0.062516	4.815333
308.730429	8000.132043	11.803456	-0.062539	4.815361
308.833210	7999.831184	11.808461	-0.062558	4.815273
308.682335	7999.920620	11.813466	-0.062530	4.815300
308.817929	7999.818102	11.818471	-0.062555	4.815269
308.752193	7999.938891	11.823475	-0.062543	4.815305
308.606846	7999.946095	11.828480	-0.062516	4.815307
308.669354	7999.841291	11.833485	-0.062527	4.815276
308.712047	8000.076146	11.838490	-0.062535	4.815345
308.629830	7999.831012	11.843495	-0.062520	4.815274
308.622981	7999.961335	11.848499	-0.062519	4.815312
308.604370	7999.919329	11.853504	-0.062515	4.815300
308.635128	7999.858901	11.858509	-0.062521	4.815282
308.519484	7999.920056	11.863514	-0.062499	4.815300
308.751950	7999.932480	11.868519	-0.062543	4.815303
308.602157	7999.967408	11.873523	-0.062515	4.815314
308.427352	7999.932424	11.878528	-0.062482	4.815304
308.592609	7999.903102	11.883533	-0.062513	4.815295
308.672468	8000.095810	11.888538	-0.062528	4.815351
308.767554	7999.934883	11.893543	-0.062546	4.815303
308.576508	7999.884661	11.898547	-0.062510	4.815290
308.695576	7999.930479	11.903552	-0.062532	4.815302
308.957873	7999.818309	11.908557	-0.062581	4.815268
308.811320	7999.907817	11.913562	-0.062554	4.815295
308.841371	7999.937185	11.918567	-0.062560	4.815304
308.813913	8000.005155	11.923571	-0.062554	4.815324
308.568688	7999.932647	11.928576	-0.062509	4.815304
308.590307	7999.930870	11.933581	-0.062513	4.815303
308.735920	7999.952539	11.938586	-0.062540	4.815309
308.806247	7999.971887	11.943591	-0.062553	4.815314
308.603940	7999.972796	11.948595	-0.062515	4.815315
308.646696	7999.957472	11.953600	-0.062523	4.815311
308.604882	7999.860553	11.958605	-0.062516	4.815282
308.578947	8000.077160	11.963610	-0.062511	4.815346
308.567379	7999.819303	11.968615	-0.062509	4.815271
308.506894	7999.817229	11.973619	-0.062497	4.815270
308.636190	7999.934849	11.978624	-0.062521	4.815304
308.565357	7999.842794	11.983629	-0.062508	4.815277
308.763689	7999.824713	11.988634	-0.062545	4.815271
308.612394	7999.801882	11.993639	-0.062517	4.815265
308.592496	7999.948024	11.998643	-0.062513	4.815308
308.513100	7999.832305	12.003648	-0.062499	4.815275
308.732666	7999.825269	12.008653	-0.062539	4.815271
308.605080	7999.907609	12.013658	-0.062516	4.815296
308.680193	7999.734590	12.018663	-0.062530	4.815245
308.735742	7999.844568	12.023667	-0.062540	4.815277
308.908116	7999.952215	12.028672	-0.062572	4.815308
308.791918	7999.917137	12.033677	-0.062551	4.815298
308.579110	7999.991643	12.038682	-0.062511	4.815321
308.699304	7999.910252	12.043687	-0.062533	4.815296
308.611481	7999.941934	12.048691	-0.062517	4.815306
308.545648	8000.008195	12.053696	-0.062505	4.815326
308.982464	7999.825160	12.058701	-0.062586	4.815270
308.845503	7999.936210	12.063706	-0.062561	4.815303
308.936518	7999.943072	12.068711	-0.062578	4.815305
308.901201	7999.838777	12.073715	-0.062571	4.815275
308.857145	7999.925715	12.078720	-0.062563	4.815300
308.891024	7999.834333	12.083725	-0.062569	4.815273
308.796910	7999.792140	12.088730	-0.062551	4.815262
308.752132	7999.958182	12.093735	-0.062543	4.815310
308.707604	7999.887947	12.098739	-0.062535	4.815290
308.756091	7999.919761	12.103744	-0.062544	4.815299
308.899439	7999.824855	12.108749	-0.062571	4.815271
308.972741	7999.982173	12.113754	-0.062584	4.815316
308.914213	7999.825103	12.118759	-0.062573	4.815271
309.017563	7999.938016	12.123763	-0.062593	4.815303
309.087145	7999.825845	12.128768	-0.062606	4.815270
309.100898	7999.736267	12.133773	-0.062608	4.815244
308.841508	7999.923327	12.138778	-0.062560	4.815300
308.790233	7999.827320	12.143783	-0.062550	4.815272
308.698372	7999.822585	12.148787	-0.062533	4.815271
308.810943	7999.838358	12.153792	-0.062554	4.815275
308.987180	7999.725825	12.158797	-0.062587	4.815241
308.878560	7999.913257	12.163802	-0.062567	4.815296
308.882384	7999.778609	12.168807	-0.062568	4.815257
309.050826	7999.962100	12.173811	-0.062599	4.815310
308.837194	7999.830246	12.178816	-0.062559	4.815272
308.885373	7999.770108	12.183821	-0.062568	4.815255
308.919881	7999.790997	12.188826	-0.062575	4.815261
309.119022	7999.916197	12.193831	-0.062612	4.815296
308.840897	7999.879492	12.198835	-0.062560	4.815287
308.787950	7999.842261	12.203840	-0.062550	4.815276
308.935089	7999.831881	12.208845	-0.062577	4.815272
308.941369	7999.908966	12.213850	-0.062579	4.815295
308.930212	7999.802935	12.218855	-0.062577	4.815264
308.881022	7999.844883	12.223859	-0.062567	4.815276
308.844185	7999.987537	12.228864	-0.062561	4.815318
308.739502	7999.843598	12.233869	-0.062541	4.815277
308.704132	7999.821627	12.238874	-0.062535	4.815271
308.783961	7999.865723	12.243879	-0.062549	4.815283
308.718173	7999.919155	12.248883	-0.062537	4.815299
308.748722	7999.851239	12.253888	-0.062543	4.815279
308.793903	7999.914002	12.258893	-0.062551	4.815297
308.759211	7999.810788	12.263898	-0.062545	4.815267
308.717558	7999.922356	12.268903	-0.062537	4.815300
308.656567	7999.877506	12.273907	-0.062526	4.815287
308.746340	7999.910007	12.278912	-0.062543	4.815296
308.760018	7999.826842	12.283917	-0.062545	4.815272
308.674593	8000.078809	12.288922	-0.062529	4.815346
308.839165	7999.840991	12.293927	-0.062560	4.815276
308.837926	7999.888014	12.298931	-0.062560	4.815289
308.929031	7999.884185	12.303936	-0.062577	4.815288
308.811216	7999.831975	12.308941	-0.062555	4.815273
308.964605	7999.974589	12.313946	-0.062583	4.815314
308.819212	7999.800036	12.318951	-0.062556	4.815264
308.831517	7999.899672	12.323955	-0.062558	4.815293
308.875348	7999.809525	12.328960	-0.062567	4.815266
309.089087	7999.745728	12.333965	-0.062606	4.815247
308.842418	7999.823947	12.338970	-0.062560	4.815271
308.858603	7999.930063	12.343975	-0.062564	4.815301
308.835658	7999.846288	12.348979	-0.062559	4.815277
308.816740	8000.079049	12.353984	-0.062556	4.815345
308.973385	7999.785503	12.358989	-0.062585	4.815259
308.959246	8000.067525	12.363994	-0.062582	4.815341
309.129255	7999.810551	12.368999	-0.062614	4.815265
309.193834	7999.952756	12.374003	-0.062626	4.815306
309.145931	8000.165793	12.379008	-0.062617	4.815369
309.239651	7999.818807	12.384013	-0.062635	4.815267
309.050372	7999.937540	12.389018	-0.062599	4.815303
309.202672	7999.942215	12.394023	-0.062628	4.815303
308.987630	8000.026307	12.399027	-0.062588	4.815329
309.003493	7999.984874	12.404032	-0.062591	4.815317
309.007026	7999.918646	12.409037	-0.062591	4.815297
308.978347	7999.983388	12.414042	-0.062586	4.815316
309.241307	7999.921480	12.419047	-0.062635	4.815297
308.875793	7999.807411	12.424051	-0.062567	4.815266
308.843032	8000.095538	12.429056	-0.062561	4.815350
309.055896	7999.907704	12.434061	-0.062600	4.815294
309.103940	8000.110576	12.439066	-0.062610	4.815353
309.111335	7999.771777	12.444071	-0.062611	4.815254
309.163893	7999.920196	12.449075	-0.062621	4.815297
309.066350	7999.839455	12.454080	-0.062602	4.815274
309.308180	7999.826376	12.459085	-0.062647	4.815269
309.319385	7999.925995	12.464090	-0.062650	4.815298
309.125629	7999.714285	12.469095	-0.062613	4.815237
309.253110	7999.923824	12.474099	-0.062637	4.815298
309.081906	7999.908145	12.479104	-0.062605	4.815294
309.224360	7999.836745	12.484109	-0.062632	4.815272
309.017532	7999.961601	12.489114	-0.062593	4.815310
309.087069	7999.794903	12.494119	-0.062606	4.815261
309.191665	7999.858656	12.499123	-0.062626	4.815279
309.193031	7999.827674	12.504128	-0.062626	4.815270
309.136228	7999.851320	12.509133	-0.062616	4.815277
309.132994	7999.794602	12.514138	-0.062615	4.815261
308.937585	7999.935685	12.519143	-0.062579	4.815303
309.119106	7999.937639	12.524147	-0.062612	4.815302
309.106460	7999.845482	12.529152	-0.062610	4.815276
309.344981	7999.886875	12.534157	-0.062654	4.815286
309.014931	7999.962636	12.539162	-0.062593	4.815310
309.064963	7999.904666	12.544167	-0.062602	4.815293
309.288047	7999.880584	12.549171	-0.062644	4.815285
309.149727	8000.050416	12.554176	-0.062618	4.815335
309.089796	8000.084702	12.559181	-0.062607	4.815345
309.254503	8000.047886	12.564186	-0.062638	4.815334
309.243208	7999.839212	12.569191	-0.062636	4.815273
309.027765	7999.798206	12.574195	-0.062595	4.815262
308.899838	7999.813184	12.579200	-0.062572	4.815267
309.341961	7999.775641	12.584205	-0.062654	4.815254
308.992888	7999.934480	12.589210	-0.062589	4.815302
309.279073	7999.883649	12.594215	-0.062642	4.815286
309.285914	7999.777918	12.599219	-0.062644	4.815255
308.955564	7999.946691	12.604224	-0.062582	4.815306
309.081937	7999.829050	12.609229	-0.062606	4.815271
309.115304	7999.951491	12.614234	-0.062612	4.815306
309.256452	7999.886485	12.619239	-0.062638	4.815287
309.208714	7999.842924	12.624243	-0.062629	4.815274
309.205023	7999.961541	12.629248	-0.062629	4.815309
309.336692	7999.835435	12.634253	-0.062653	4.815271
309.179428	7999.871307	12.639258	-0.062624	4.815283
309.075195	7999.913408	12.644263	-0.062604	4.815296
309.105466	7999.879699	12.649267	-0.062610	4.815286
309.054558	8000.053126	12.654272	-0.062601	4.815336
309.209070	7999.822623	12.659277	-0.062629	4.815268
309.190122	7999.831930	12.664282	-0.062626	4.815271
309.118855	7999.871373	12.669287	-0.062613	4.815283
309.094907	7999.819655	12.674291	-0.062608	4.815268
309.055919	7999.940891	12.679296	-0.062601	4.815304
309.366803	7999.786763	12.684301	-0.062659	4.815257
309.183957	7999.886359	12.689306	-0.062625	4.815287
309.251346	7999.921695	12.694311	-0.062637	4.815297
309.329150	7999.878087	12.699315	-0.062652	4.815284
309.152845	7999.710503	12.704320	-0.062619	4.815236
309.347981	7999.827082	12.709325	-0.062655	4.815269
309.147062	7999.940276	12.714330	-0.062618	4.815303
309.307031	7999.947218	12.719335	-0.062648	4.815304
309.209754	7999.827991	12.724339	-0.062630	4.815270
309.294702	7999.958775	12.729344	-0.062646	4.815308
309.416390	7999.944765	12.734349	-0.062668	4.815303
309.269811	8000.109115	12.739354	-0.062641	4.815352
309.272640	7999.817281	12.744359	-0.062641	4.815267
309.283971	7999.925456	12.749363	-0.062644	4.815298
309.173915	7999.924693	12.754368	-0.062623	4.815298
309.157522	7999.817505	12.759373	-0.062620	4.815267
309.148200	7999.816282	12.764378	-0.062618	4.815267
309.204541	7999.841811	12.769383	-0.062629	4.815274
309.125325	7999.936717	12.774387	-0.062614	4.815302
309.162693	7999.829356	12.779392	-0.062621	4.815271
309.413475	7999.848500	12.784397	-0.062668	4.815275
309.297916	7999.974876	12.789402	-0.062646	4.815312
309.125859	7999.933522	12.794407	-0.062614	4.815301
309.308095	7999.858509	12.799411	-0.062648	4.815278
309.320523	7999.915382	12.804416	-0.062650	4.815295
309.329254	7999.808613	12.809421	-0.062652	4.815264
309.370689	7999.856346	12.814426	-0.062660	4.815277
309.308434	7999.851034	12.819431	-0.062648	4.815276
309.183673	7999.784808	12.824435	-0.062625	4.815257
308.944668	7999.821458	12.829440	-0.062580	4.815269
309.098997	7999.755603	12.834445	-0.062609	4.815249
309.077792	7999.960528	12.839450	-0.062605	4.815309
309.080127	7999.749945	12.844455	-0.062606	4.815248
309.136828	7999.822522	12.849459	-0.062616	4.815269
309.147336	7999.814145	12.854464	-0.062618	4.815266
308.973460	7999.820874	12.859469	-0.062586	4.815269
309.019311	7999.849436	12.864474	-0.062594	4.815277
309.285965	7999.832493	12.869479	-0.062644	4.815271
309.342179	7999.841983	12.874483	-0.062655	4.815273
309.347380	7999.837794	12.879488	-0.062656	4.815272
309.494857	7999.768617	12.884493	-0.062683	4.815251
309.145941	7999.777777	12.889498	-0.062618	4.815256
309.050206	7999.824296	12.894503	-0.062600	4.815270
309.302736	7999.883028	12.899507	-0.062647	4.815286
309.133717	7999.834241	12.904512	-0.062616	4.815272
309.092023	7999.748016	12.909517	-0.062608	4.815247
309.162683	7999.859316	12.914522	-0.062621	4.815279
309.370558	7999.869192	12.919527	-0.062660	4.815281
309.379232	7999.778459	12.924531	-0.062662	4.815255
308.941457	7999.838529	12.929536	-0.062580	4.815274
309.204839	7999.940208	12.934541	-0.062629	4.815303
309.273696	7999.900727	12.939546	-0.062642	4.815291
309.345182	7999.813178	12.944551	-0.062655	4.815265
309.320999	7999.858750	12.949555	-0.062651	4.815278
309.411583	7999.808940	12.954560	-0.062668	4.815263
309.437446	7999.814717	12.959565	-0.062672	4.815265
309.399667	7999.912452	12.964570	-0.062666	4.815294
309.232310	7999.823064	12.969575	-0.062634	4.815268
309.246998	7999.780543	12.974579	-0.062637	4.815256
309.192329	7999.853406	12.979584	-0.062627	4.815277
309.547336	7999.765231	12.984589	-0.062693	4.815250
309.409249	7999.951106	12.989594	-0.062667	4.815305
309.350557	7999.818622	12.994599	-0.062656	4.815267
309.342712	7999.866605	12.999603	-0.062655	4.815281
309.347618	7999.939390	13.004608	-0.062656	4.815302
309.376588	7999.918490	13.009613	-0.062661	4.815296
309.443980	7999.975210	13.014618	-0.062674	4.815312
309.480592	7999.806893	13.019623	-0.062681	4.815262
309.547584	7999.835807	13.024627	-0.062693	4.815271
309.342957	7999.938248	13.029632	-0.062655	4.815301
309.473637	7999.750114	13.034637	-0.062679	4.815246
309.633228	7999.865034	13.039642	-0.062709	4.815279
309.472192	7999.908328	13.044647	-0.062679	4.815292
309.481783	7999.825093	13.049651	-0.062681	4.815268
309.508822	7999.809507	13.054656	-0.062686	4.815263
309.586035	7999.837523	13.059661	-0.062700	4.815271
309.227834	7999.812315	13.064666	-0.062634	4.815265
309.241995	7999.823243	13.069671	-0.062636	4.815268
309.300376	7999.864844	13.074675	-0.062647	4.815280
309.326763	7999.863146	13.079680	-0.062652	4.815280
309.445902	7999.821295	13.084685	-0.062674	4.815267
309.422276	8000.036874	13.089690	-0.062670	4.815330
309.517494	7999.980725	13.094695	-0.062688	4.815313
309.448192	7999.937874	13.099699	-0.062675	4.815301
309.472996	7999.976778	13.104704	-0.062679	4.815312
309.405333	7999.862321	13.109709	-0.062667	4.815279
309.440114	8000.014723	13.114714	-0.062673	4.815323
309.505602	7999.822295	13.119719	-0.062685	4.815267
309.503450	7999.830813	13.124723	-0.062685	4.815269
309.280305	7999.924392	13.129728	-0.062644	4.815298
309.442519	7999.896088	13.134733	-0.062674	4.815289
309.469015	7999.945712	13.139738	-0.062679	4.815303
309.420633	7999.839060	13.144743	-0.062670	4.815272
309.381663	7999.745396	13.149747	-0.062662	4.815245
309.428005	8000.082955	13.154752	-0.062671	4.815343
309.592588	7999.729664	13.159757	-0.062702	4.815239
309.311821	7999.804108	13.164762	-0.062649	4.815262
309.478492	7999.931976	13.169767	-0.062681	4.815299
309.653827	7999.837603	13.174771	-0.062713	4.815271
309.536989	8000.045215	13.179776	-0.062692	4.815332
309.304750	7999.997512	13.184781	-0.062648	4.815319
309.614175	7999.983421	13.189786	-0.062706	4.815313
309.466863	7999.840908	13.194791	-0.062678	4.815272
309.417916	7999.843301	13.199795	-0.062669	4.815273
309.342869	7999.997081	13.204800	-0.062655	4.815319
309.565298	7999.830789	13.209805	-0.062697	4.815269
309.255771	7999.761487	13.214810	-0.062639	4.815250
309.352980	7999.997252	13.219815	-0.062657	4.815319
309.614195	7999.879718	13.224819	-0.062706	4.815283
309.645885	7999.934774	13.229824	-0.062712	4.815299
309.416038	7999.810132	13.234829	-0.062669	4.815264
309.497955	7999.826465	13.239834	-0.062684	4.815268
309.505731	7999.984832	13.244839	-0.062686	4.815314
309.653358	7999.850438	13.249843	-0.062713	4.815274
309.510540	7999.928248	13.254848	-0.062687	4.815298
309.602662	7999.828212	13.259853	-0.062704	4.815268
309.585129	7999.807607	13.264858	-0.062701	4.815262
309.346580	7999.930866	13.269863	-0.062656	4.815299
309.516998	7999.871693	13.274867	-0.062688	4.815281
309.305222	8000.070240	13.279872	-0.062649	4.815340
309.428418	7999.812485	13.284877	-0.062671	4.815264
309.522314	8000.103795	13.289882	-0.062689	4.815349
309.457541	7999.994730	13.294887	-0.062677	4.815317
309.430812	7999.794352	13.299891	-0.062672	4.815259
309.344482	7999.975742	13.304896	-0.062656	4.815312
309.485664	7999.886146	13.309901	-0.062682	4.815286
309.341296	7999.935063	13.314906	-0.062655	4.815301
309.267305	7999.952007	13.319911	-0.062642	4.815306
309.594802	7999.827024	13.324915	-0.062703	4.815268
309.568201	7999.934567	13.329920	-0.062698	4.815299
309.529927	7999.724375	13.334925	-0.062690	4.815238
309.356900	7999.937465	13.339930	-0.062658	4.815301
309.440535	7999.994456	13.344935	-0.062674	4.815317
309.484313	7999.979148	13.349939	-0.062682	4.815313
309.418926	7999.940639	13.354944	-0.062670	4.815302
309.590324	7999.923180	13.359949	-0.062702	4.815296
309.405026	7999.967139	13.364954	-0.062667	4.815310
309.443812	7999.933572	13.369959	-0.062675	4.815300
309.605056	7999.965126	13.374963	-0.062705	4.815308
309.407251	7999.854916	13.379968	-0.062668	4.815277
309.366766	7999.857450	13.384973	-0.062660	4.815278
309.436823	7999.983710	13.389978	-0.062673	4.815314
309.448166	7999.946479	13.394983	-0.062675	4.815303
309.553181	7999.838105	13.399987	-0.062695	4.815271
309.506199	8000.035119	13.404992	-0.062686	4.815329
309.518110	7999.857836	13.409997	-0.062688	4.815277
309.380453	7999.950701	13.415002	-0.062663	4.815305
309.235925	7999.948295	13.420007	-0.062636	4.815305
309.507915	7999.903643	13.425011	-0.062687	4.815291
309.400635	8000.060095	13.430016	-0.062667	4.815337
309.318571	7999.898354	13.435021	-0.062651	4.815290
309.356676	7999.977038	13.440026	-0.062658	4.815313
309.405371	7999.844205	13.445031	-0.062667	4.815274
309.546796	7999.767442	13.450035	-0.062694	4.815251
309.372718	7999.951648	13.455040	-0.062661	4.815305
309.438285	7999.834064	13.460045	-0.062674	4.815271
309.577801	7999.816073	13.465050	-0.062700	4.815265
309.365423	7999.932284	13.470055	-0.062660	4.815300
309.390355	7999.867481	13.475059	-0.062665	4.815281
309.485078	8000.012328	13.480064	-0.062682	4.815322
309.455700	7999.820459	13.485069	-0.062677	4.815267
309.450288	7999.989298	13.490074	-0.062676	4.815316
309.478228	7999.828320	13.495079	-0.062681	4.815269
309.493546	7999.830714	13.500083	-0.062684	4.815269
309.478220	7999.950206	13.505088	-0.062681	4.815304
309.426324	7999.822112	13.510093	-0.062671	4.815267
309.410052	7999.882785	13.515098	-0.062669	4.815285
309.295369	7999.848801	13.520103	-0.062647	4.815276
309.541492	7999.829379	13.525107	-0.062693	4.815269
309.531226	7999.955370	13.530112	-0.062691	4.815306
309.606668	7999.942728	13.535117	-0.062705	4.815301
309.493550	7999.963298	13.540122	-0.062684	4.815308
309.441557	8000.027652	13.545127	-0.062675	4.815327
309.407748	7999.941556	13.550131	-0.062668	4.815302
309.426055	8000.055194	13.555136	-0.062672	4.815335
309.495499	7999.930190	13.560141	-0.062685	4.815298
309.521837	8000.062137	13.565146	-0.062690	4.815337
309.511613	7999.981780	13.570151	-0.062688	4.815313
309.549482	7999.813483	13.575155	-0.062695	4.815264
309.619980	7999.798620	13.580160	-0.062708	4.815259
309.614741	7999.888344	13.585165	-0.062707	4.815286
309.711332	7999.881400	13.590170	-0.062725	4.815283
309.594756	7999.954301	13.595175	-0.062703	4.815305
309.456417	7999.732820	13.600179	-0.062677	4.815241
309.444093	7999.930411	13.605184	-0.062675	4.815299
309.539292	7999.827219	13.610189	-0.062693	4.815268
309.646044	7999.836481	13.615194	-0.062713	4.815270
309.535710	7999.937285	13.620199	-0.062692	4.815300
309.572063	7999.760410	13.625203	-0.062699	4.815248
309.615890	7999.948244	13.630208	-0.062707	4.815303
309.575913	7999.970032	13.635213	-0.062700	4.815310
309.576474	7999.832120	13.640218	-0.062700	4.815269
309.496540	7999.945190	13.645223	-0.062685	4.815303
309.642740	7999.866369	13.650227	-0.062712	4.815279
309.250435	7999.929333	13.655232	-0.062639	4.815299
309.331724	7999.878298	13.660237	-0.062654	4.815284
309.371217	7999.889648	13.665242	-0.062662	4.815287
309.348350	7999.955557	13.670247	-0.062657	4.815306
309.440125	7999.812749	13.675251	-0.062674	4.815264
309.453369	7999.935924	13.680256	-0.062677	4.815300
309.511626	7999.848154	13.685261	-0.062688	4.815274
309.384115	7999.834271	13.690266	-0.062664	4.815271
309.275061	7999.958617	13.695271	-0.062644	4.815308
309.384720	7999.923024	13.700275	-0.062664	4.815297
309.235731	7999.967587	13.705280	-0.062636	4.815311
309.356371	7999.773940	13.710285	-0.062659	4.815253
309.478687	7999.879686	13.715290	-0.062682	4.815284
309.484027	7999.970655	13.720295	-0.062683	4.815310
309.493162	7999.740938	13.725299	-0.062684	4.815243
309.458691	7999.859042	13.730304	-0.062678	4.815278
309.317871	7999.927262	13.735309	-0.062652	4.815298
309.483988	7999.831666	13.740314	-0.062683	4.815270
309.381716	7999.829964	13.745319	-0.062664	4.815270
309.660973	7999.939394	13.750323	-0.062716	4.815300
309.290337	7999.979196	13.755328	-0.062647	4.815314
309.669943	7999.824075	13.760333	-0.062717	4.815267
309.500734	7999.934589	13.765338	-0.062686	4.815300
309.464095	7999.930773	13.770343	-0.062679	4.815299
309.395759	7999.903976	13.775347	-0.062666	4.815291
309.457392	7999.922109	13.780352	-0.062678	4.815296
309.413171	7999.928858	13.785357	-0.062670	4.815298
309.560876	7999.876791	13.790362	-0.062697	4.815282
309.749553	7999.930185	13.795367	-0.062732	4.815297
309.797878	7999.813382	13.800371	-0.062741	4.815263
309.648922	7999.930649	13.805376	-0.062714	4.815298
309.748257	7999.985764	13.810381	-0.062732	4.815313
309.695050	7999.910036	13.815386	-0.062722	4.815291
309.542966	7999.820902	13.820391	-0.062694	4.815266
309.643580	7999.809748	13.825395	-0.062713	4.815262
309.825225	7999.843779	13.830400	-0.062746	4.815271
309.506043	7999.928275	13.835405	-0.062687	4.815298
309.671711	7999.796320	13.840410	-0.062718	4.815258
309.706388	8000.001110	13.845415	-0.062724	4.815318
309.755330	7999.730357	13.850419	-0.062733	4.815239
309.484979	7999.830634	13.855424	-0.062683	4.815269
309.479223	7999.843369	13.860429	-0.062682	4.815273
309.643117	7999.828992	13.865434	-0.062713	4.815268
309.534258	7999.935166	13.870439	-0.062692	4.815300
309.623076	7999.806208	13.875443	-0.062709	4.815262
309.459151	7999.739330	13.880448	-0.062678	4.815243
309.558025	7999.821164	13.885453	-0.062697	4.815266
309.594603	7999.872025	13.890458	-0.062704	4.815281
309.491795	7999.716354	13.895463	-0.062684	4.815236
309.485836	7999.801789	13.900467	-0.062683	4.815261
309.527242	7999.932917	13.905472	-0.062691	4.815299
309.520655	7999.823753	13.910477	-0.062690	4.815267
309.635501	7999.855603	13.915482	-0.062711	4.815276
309.606752	7999.948143	13.920487	-0.062706	4.815303
309.592504	7999.819607	13.925491	-0.062703	4.815266
309.532326	7999.849611	13.930496	-0.062692	4.815275
309.546599	7999.918276	13.935501	-0.062695	4.815295
309.603932	7999.802693	13.940506	-0.062705	4.815261
309.563305	8000.062895	13.945511	-0.062698	4.815337
309.654993	7999.727634	13.950515	-0.062715	4.815238
309.491854	7999.930198	13.955520	-0.062685	4.815298
309.449284	7999.877101	13.960525	-0.062677	4.815283
309.374506	7999.916485	13.965530	-0.062663	4.815295
309.511081	7999.915553	13.970535	-0.062688	4.815294
309.557988	7999.814764	13.975539	-0.062697	4.815264
309.432703	7999.943117	13.980544	-0.062674	4.815302
309.673373	7999.797442	13.985549	-0.062718	4.815259
309.864418	7999.847668	13.990554	-0.062754	4.815272
309.561246	7999.938845	13.995559	-0.062698	4.815301
309.853815	7999.822902	14.000563	-0.062752	4.815265
309.632751	7999.943245	14.005568	-0.062711	4.815301
309.622774	7999.837232	14.010573	-0.062709	4.815271
309.397649	7999.927571	14.015578	-0.062667	4.815298
309.578422	7999.829011	14.020583	-0.062701	4.815268
309.431304	7999.825493	14.025587	-0.062673	4.815268
309.603316	7999.984457	14.030592	-0.062706	4.815314
309.866997	7999.903316	14.035597	-0.062755	4.815289
309.710654	7999.848323	14.040602	-0.062725	4.815273
309.581223	8000.008683	14.045607	-0.062702	4.815321
309.756921	7999.825574	14.050611	-0.062734	4.815267
309.770427	7999.829007	14.055616	-0.062737	4.815267
309.578647	7999.838645	14.060621	-0.062701	4.815271
309.696764	7999.826713	14.065626	-0.062723	4.815267
309.614805	7999.844594	14.070631	-0.062708	4.815273
309.747694	7999.804041	14.075635	-0.062732	4.815260
309.557389	7999.976217	14.080640	-0.062697	4.815311
309.618614	7999.878874	14.085645	-0.062708	4.815283
309.715621	7999.932879	14.090650	-0.062727	4.815298
309.716092	7999.970309	14.095655	-0.062727	4.815309
309.897407	8000.016098	14.100659	-0.062760	4.815321
309.657960	7999.961859	14.105664	-0.062716	4.815307
309.649517	8000.083605	14.110669	-0.062714	4.815342
309.590884	7999.851688	14.115674	-0.062703	4.815275
309.615790	7999.929084	14.120679	-0.062708	4.815297
309.611789	7999.859522	14.125683	-0.062707	4.815277
309.482226	7999.907616	14.130688	-0.062683	4.815292
309.654182	7999.843123	14.135693	-0.062715	4.815272
309.589591	7999.853809	14.140698	-0.062703	4.815276
309.406629	7999.919190	14.145703	-0.062669	4.815296
309.539132	8000.056113	14.150707	-0.062694	4.815335
309.498624	7999.975251	14.155712	-0.062686	4.815311
309.511550	7999.964776	14.160717	-0.062689	4.815308
309.605521	7999.972757	14.165722	-0.062706	4.815310
309.596355	7999.829336	14.170727	-0.062704	4.815268
309.775994	7999.897548	14.175731	-0.062738	4.815287
309.704364	7999.943400	14.180736	-0.062725	4.815301
309.740242	7999.812490	14.185741	-0.062731	4.815263
309.962645	7999.840785	14.190746	-0.062773	4.815270
309.729377	7999.840109	14.195751	-0.062729	4.815271
309.670864	7999.798507	14.200755	-0.062718	4.815259
309.610810	7999.935431	14.205760	-0.062707	4.815299
309.711368	7999.835535	14.210765	-0.062726	4.815270
309.845645	7999.914753	14.215770	-0.062751	4.815292
309.745288	7999.964403	14.220775	-0.062732	4.815307
309.827579	7999.888793	14.225779	-0.062748	4.815285
309.640556	7999.849328	14.230784	-0.062713	4.815274
309.672318	7999.958913	14.235789	-0.062719	4.815306
309.774926	8000.014082	14.240794	-0.062738	4.815321
309.692908	8000.011648	14.245799	-0.062723	4.815321
309.470986	7999.493688	14.250803	-0.062681	4.815171
309.592727	7996.350597	14.255808	-0.062702	4.814252
309.655967	7990.722501	14.260813	-0.062710	4.812608
309.581209	7983.989581	14.265818	-0.062691	4.810641
309.569966	7976.662568	14.270823	-0.062685	4.808499
309.483551	7969.031359	14.275827	-0.062664	4.806267
309.555391	7961.207822	14.280832	-0.062672	4.803978
309.621264	7953.330334	14.285837	-0.062679	4.801671
309.632708	7945.404629	14.290842	-0.062676	4.799350
309.556637	7937.445226	14.295847	-0.062657	4.797017
309.263909	7929.402390	14.300851	-0.062597	4.794661
309.471186	7921.386966	14.305856	-0.062630	4.792309
309.354373	7913.353673	14.310861	-0.062603	4.789951
309.233797	7905.407247	14.315866	-0.062576	4.787619
309.221276	7897.345158	14.320871	-0.062568	4.785250
309.322697	7889.408666	14.325875	-0.062582	4.782917
309.425225	7881.410223	14.330880	-0.062596	4.780565
309.355168	7873.386819	14.335885	-0.062577	4.778205
309.373558	7865.422679	14.340890	-0.062576	4.775860
309.193205	7857.384577	14.345895	-0.062537	4.773494
309.107615	7849.367661	14.350899	-0.062516	4.771132
309.380109	7841.372051	14.355904	-0.062561	4.768774
309.209477	7833.348251	14.360909	-0.062524	4.766408
309.079149	7825.418918	14.365914	-0.062495	4.764069
308.864717	7817.394186	14.370919	-0.062450	4.761700
309.071806	7809.372273	14.375923	-0.062483	4.759330
308.956891	7801.410672	14.380928	-0.062456	4.756978
309.002885	7793.314537	14.385933	-0.062460	4.754584
308.791518	7785.319758	14.390938	-0.062415	4.752220
308.763204	7777.248851	14.395943	-0.062405	4.749831
308.693204	7769.366020	14.400947	-0.062387	4.747497
308.781252	7761.290757	14.405952	-0.062398	4.745104
308.667450	7753.362700	14.410957	-0.062371	4.742755
308.696335	7745.296983	14.415962	-0.062371	4.740362
308.558358	7737.299890	14.420967	-0.062341	4.737990
308.870405	7729.320872	14.425971	-0.062393	4.735620
308.482823	7721.305177	14.430976	-0.062316	4.733241
308.342114	7713.287666	14.435981	-0.062285	4.730859
308.447262	7705.334335	14.440986	-0.062299	4.728494
308.268560	7697.251145	14.445991	-0.062261	4.726090
308.251591	7689.351908	14.450995	-0.062252	4.723739
308.308543	7681.328347	14.456000	-0.062258	4.721350
308.384979	7673.292242	14.461005	-0.062267	4.718956
308.396544	7665.376922	14.466010	-0.062264	4.716596
308.295900	7657.289841	14.471015	-0.062240	4.714185
308.358820	7649.312890	14.476019	-0.062246	4.711805
308.346691	7641.318445	14.481024	-0.062239	4.709418
308.171194	7633.284994	14.486029	-0.062201	4.707019
308.316897	7625.271728	14.491034	-0.062223	4.704624
308.276543	7617.287219	14.496039	-0.062210	4.702237
308.164899	7609.259322	14.501043	-0.062184	4.699836
308.208443	7601.331569	14.506048	-0.062187	4.697463
308.017433	7593.284260	14.511053	-0.062146	4.695054
308.067712	7585.243800	14.516058	-0.062150	4.692645
307.898432	7577.245619	14.521063	-0.062114	4.690248
308.104601	7569.307016	14.526067	-0.062147	4.687867
308.174183	7561.252966	14.531072	-0.062155	4.685450
308.023477	7553.292220	14.536077	-0.062121	4.683061
308.045112	7545.291893	14.541082	-0.062120	4.680658
308.003571	7537.272480	14.546087	-0.062107	4.678248
307.940888	7529.290332	14.551091	-0.062090	4.675848
307.903507	7521.190012	14.556096	-0.062078	4.673411
307.873364	7513.162418	14.561101	-0.062067	4.670995
307.918898	7505.220195	14.566106	-0.062071	4.668603
307.516525	7497.171254	14.571111	-0.061990	4.666179
307.737926	7489.267040	14.576115	-0.062026	4.663796
307.867380	7481.195661	14.581120	-0.062045	4.661361
307.562564	7473.215716	14.586125	-0.061983	4.658953
307.610309	7465.293017	14.591130	-0.061987	4.656561
307.692591	7457.225713	14.596135	-0.061997	4.654124
307.640656	7449.211736	14.601139	-0.061982	4.651702
307.538378	7441.180129	14.606144	-0.061958	4.649274
307.466055	7433.212688	14.611149	-0.061939	4.646863
307.580642	7425.204561	14.616154	-0.061956	4.644439
307.370929	7417.216244	14.621159	-0.061911	4.642020
307.604698	7409.199233	14.626163	-0.061950	4.639590
307.354213	7401.242945	14.631168	-0.061898	4.637178
307.252069	7393.172867	14.636173	-0.061874	4.634730
307.235783	7385.205977	14.641178	-0.061865	4.632312
307.378039	7377.129420	14.646183	-0.061887	4.629859
307.465594	7369.187488	14.651187	-0.061898	4.627446
307.271398	7361.144610	14.656192	-0.061856	4.625002
307.189119	7353.192380	14.661197	-0.061836	4.622583
307.369440	7345.168663	14.666202	-0.061864	4.620141
307.111799	7337.206269	14.671207	-0.061811	4.617717
307.322163	7329.192004	14.676211	-0.061845	4.615276
307.416995	7321.176762	14.681216	-0.061857	4.612833
307.255740	7313.123768	14.686221	-0.061822	4.610377
307.220251	7305.186616	14.691226	-0.061810	4.607955
307.016787	7297.149433	14.696231	-0.061767	4.605502
307.065628	7289.205383	14.701235	-0.061771	4.603075
306.956445	7281.177796	14.706240	-0.061746	4.600622
307.023820	7273.170707	14.711245	-0.061753	4.598174
307.066632	7265.175035	14.716250	-0.061756	4.595728
306.932203	7257.084938	14.721255	-0.061725	4.593251
306.883444	7249.069455	14.726259	-0.061711	4.590796
306.972204	7241.104904	14.731264	-0.061722	4.588356
306.804049	7233.114516	14.736269	-0.061686	4.585906
306.706972	7225.153758	14.741274	-0.061663	4.583464
306.724327	7217.118720	14.746279	-0.061661	4.580998
306.682154	7209.107471	14.751283	-0.061648	4.578538
306.659160	7201.125898	14.756288	-0.061638	4.576085
306.559435	7193.098076	14.761293	-0.061614	4.573618
306.699799	7185.120575	14.766298	-0.061635	4.571164
306.552977	7177.105653	14.771303	-0.061603	4.568697
306.459926	7169.117240	14.776307	-0.061580	4.566237
306.551293	7161.141619	14.781312	-0.061592	4.563780
306.361868	7153.127807	14.786317	-0.061552	4.561310
306.323410	7145.148169	14.791322	-0.061539	4.558849
306.176791	7137.150058	14.796327	-0.061507	4.556381
306.307597	7129.133887	14.801331	-0.061526	4.553906
306.372234	7121.093038	14.806336	-0.061533	4.551422
306.196097	7113.077918	14.811341	-0.061495	4.548944
306.164110	7105.090741	14.816346	-0.061484	4.546474
306.095671	7097.099037	14.821351	-0.061466	4.544001
306.002990	7089.132012	14.826355	-0.061443	4.541535
305.995309	7081.094323	14.831360	-0.061436	4.539045
306.013491	7073.122335	14.836365	-0.061435	4.536574
305.992214	7065.106616	14.841370	-0.061426	4.534088
306.103755	7057.085435	14.846375	-0.061441	4.531600
306.139530	7049.087205	14.851379	-0.061443	4.529117
306.117584	7041.127899	14.856384	-0.061433	4.526645
306.034336	7033.055871	14.861389	-0.061413	4.524136
306.117410	7025.158842	14.866394	-0.061423	4.521680
306.133745	7017.070937	14.871399	-0.061421	4.519164
305.818094	7009.140366	14.876403	-0.061357	4.516694
305.923549	7001.061785	14.881408	-0.061371	4.514178
305.671857	6993.001452	14.886413	-0.061319	4.511666
305.618806	6985.044236	14.891418	-0.061304	4.509184
305.704846	6977.011270	14.896423	-0.061315	4.506678
305.757356	6969.007022	14.901427	-0.061319	4.504180
305.459665	6961.102113	14.906432	-0.061259	4.501710
305.667620	6953.042468	14.911437	-0.061292	4.499192
305.720688	6945.103428	14.916442	-0.061297	4.496710
305.589181	6937.046732	14.921447	-0.061267	4.494188
305.484097	6929.008330	14.926451	-0.061242	4.491672
305.596336	6921.012284	14.931456	-0.061258	4.489168
305.730351	6913.022446	14.936461	-0.061278	4.486664
305.605127	6905.034601	14.941466	-0.061249	4.484159
305.560135	6897.080316	14.946471	-0.061236	4.481663
305.465671	6889.031568	14.951475	-0.061213	4.479136
305.276319	6881.056964	14.956480	-0.061173	4.476631
305.356444	6873.014522	14.961485	-0.061182	4.474104
305.413457	6865.003650	14.966490	-0.061188	4.471585
305.520564	6856.947126	14.971495	-0.061202	4.469050
305.383620	6849.021805	14.976499	-0.061172	4.466555
305.190346	6840.992621	14.981504	-0.061130	4.464025
305.099541	6833.051061	14.986509	-0.061108	4.461522
305.241832	6825.046917	14.991514	-0.061130	4.458999
305.070636	6817.012437	14.996519	-0.061093	4.456463
305.179368	6809.007866	15.001523	-0.061108	4.453936
305.229749	6801.005559	15.006528	-0.061112	4.451409
305.040524	6792.972286	15.011533	-0.061071	4.448869
305.062196	6785.006129	15.016538	-0.061070	4.446350
304.901422	6777.010354	15.021543	-0.061035	4.443819
305.051085	6769.003293	15.026547	-0.061058	4.441285
305.080430	6761.008269	15.031552	-0.061058	4.438752
305.021071	6752.974695	15.036557	-0.061042	4.436205
305.081209	6744.976600	15.041562	-0.061048	4.433669
304.789083	6736.919124	15.046567	-0.060988	4.431111
305.042518	6728.934410	15.051571	-0.061030	4.428577
305.119679	6720.960628	15.056576	-0.061039	4.426044
304.841701	6712.970030	15.061581	-0.060982	4.423503
305.055731	6704.956302	15.066586	-0.061017	4.420955
304.934828	6696.968778	15.071591	-0.060989	4.418412
304.626353	6688.978936	15.076595	-0.060927	4.415866
304.645797	6680.968249	15.081600	-0.060925	4.413314
304.442413	6672.938234	15.086605	-0.060882	4.410753
304.569677	6664.990956	15.091610	-0.060900	4.408219
304.404999	6656.913003	15.096615	-0.060864	4.405640
304.565575	6648.961679	15.101619	-0.060889	4.403101
304.417485	6640.957390	15.106624	-0.060856	4.400543
304.366769	6632.976721	15.111629	-0.060842	4.397991
304.537957	6624.995069	15.116634	-0.060868	4.395438
304.446484	6616.960012	15.121639	-0.060846	4.392866
304.273034	6608.910640	15.126643	-0.060809	4.390287
304.371411	6600.960730	15.131648	-0.060822	4.387739
304.341764	6592.903756	15.136653	-0.060811	4.385156
304.418822	6584.996557	15.141658	-0.060820	4.382619
304.129310	6576.933224	15.146663	-0.060761	4.380029
304.158525	6569.012844	15.151667	-0.060761	4.377485
304.196058	6560.991073	15.156672	-0.060763	4.374906
304.014138	6552.944091	15.161677	-0.060724	4.372317
304.009937	6544.929691	15.166682	-0.060718	4.369738
304.007031	6536.972350	15.171687	-0.060712	4.367176
303.890688	6528.939498	15.176691	-0.060685	4.364587
304.010327	6521.029900	15.181696	-0.060703	4.362038
304.007381	6512.949223	15.186701	-0.060697	4.359432
304.091078	6505.046723	15.191706	-0.060707	4.356882
303.794403	6496.956279	15.196711	-0.060647	4.354267
303.764369	6488.845225	15.201715	-0.060636	4.351646
303.785032	6480.860646	15.206720	-0.060635	4.349064
303.795209	6472.832786	15.211725	-0.060631	4.346467
303.805332	6464.925423	15.216730	-0.060628	4.343907
303.593217	6456.972405	15.221735	-0.060583	4.341330
303.639675	6448.945613	15.226739	-0.060587	4.338728
303.542348	6440.973814	15.231744	-0.060563	4.336142
303.531646	6432.923219	15.236749	-0.060556	4.333530
303.495030	6424.904002	15.241754	-0.060544	4.330926
303.355341	6416.916841	15.246759	-0.060513	4.328330
303.228467	6408.936176	15.251763	-0.060484	4.325735
303.639439	6400.957128	15.256768	-0.060555	4.323142
303.452790	6392.928886	15.261773	-0.060515	4.320528
303.569888	6384.974476	15.266778	-0.060532	4.317938
303.538662	6376.904607	15.271783	-0.060521	4.315308
303.418675	6368.917322	15.276787	-0.060493	4.312703
303.191376	6360.908693	15.281792	-0.060446	4.310088
303.098132	6352.878009	15.286797	-0.060423	4.307466
303.210899	6344.933425	15.291802	-0.060439	4.304871
302.948584	6336.928927	15.296807	-0.060385	4.302253
303.029384	6328.881167	15.301811	-0.060395	4.299621
303.093121	6320.962698	15.306816	-0.060402	4.297030
303.023402	6312.887329	15.311821	-0.060383	4.294385
302.965284	6304.903367	15.316826	-0.060367	4.291769
302.898377	6296.885493	15.321831	-0.060350	4.289139
302.946384	6288.903019	15.326835	-0.060353	4.286521
302.893421	6280.935539	15.331840	-0.060338	4.283905
302.823259	6272.882171	15.336845	-0.060320	4.281259
302.831123	6264.923949	15.341850	-0.060316	4.278644
302.805686	6256.906916	15.346855	-0.060306	4.276007
302.909436	6248.896264	15.351859	-0.060321	4.273371
302.829586	6240.848837	15.356864	-0.060300	4.270721
302.745705	6232.830233	15.361869	-0.060280	4.268078
302.772512	6224.871469	15.366874	-0.060279	4.265454
302.724813	6216.859973	15.371879	-0.060265	4.262811
302.722652	6208.861711	15.376883	-0.060260	4.260171
302.797276	6200.923988	15.381888	-0.060268	4.257549
302.615954	6192.878142	15.386893	-0.060230	4.254889
302.716043	6184.895788	15.391898	-0.060243	4.252249
302.421658	6176.862239	15.396903	-0.060183	4.249588
302.551648	6168.929550	15.401907	-0.060202	4.246963
302.558915	6160.894935	15.406912	-0.060198	4.244301
302.337587	6152.879313	15.411917	-0.060152	4.241641
302.452127	6144.884725	15.416922	-0.060168	4.238990
302.309834	6136.945655	15.421927	-0.060136	4.236353
302.356736	6128.874633	15.426931	-0.060140	4.233672
302.168674	6120.868070	15.431936	-0.060099	4.231009
302.290019	6112.867971	15.436941	-0.060117	4.228350
302.381306	6104.900001	15.441946	-0.060129	4.225699
302.079856	6096.916692	15.446951	-0.060067	4.223037
302.139382	6088.913806	15.451955	-0.060073	4.220371
302.302307	6080.942831	15.456960	-0.060098	4.217715
302.052428	6072.888179	15.461965	-0.060047	4.215025
302.072849	6064.905402	15.466970	-0.060045	4.212360
301.844285	6056.853965	15.471975	-0.059997	4.209668
301.920501	6048.932899	15.476979	-0.060006	4.207021
301.739270	6040.951010	15.481984	-0.059967	4.204349
301.814435	6032.933699	15.486989	-0.059976	4.201666
301.987424	6024.916574	15.491994	-0.060003	4.198983
301.913950	6016.926208	15.496999	-0.059984	4.196304
301.803332	6008.874217	15.502003	-0.059959	4.193603
301.858491	6000.771981	15.507008	-0.059964	4.190884
301.769875	5992.833868	15.512013	-0.059942	4.188218
301.707631	5984.853564	15.517018	-0.059925	4.185536
301.742831	5976.884540	15.522023	-0.059926	4.182857
301.656890	5968.878172	15.527027	-0.059905	4.180162
301.783752	5960.896004	15.532032	-0.059924	4.177476
301.444184	5952.867571	15.537037	-0.059855	4.174768
301.824233	5944.883631	15.542042	-0.059921	4.172081
301.442977	5936.842137	15.547047	-0.059845	4.169364
301.519178	5928.865624	15.552051	-0.059854	4.166673
301.725532	5920.874148	15.557056	-0.059887	4.163976
301.717433	5912.910737	15.562061	-0.059880	4.161284
301.456684	5904.930641	15.567066	-0.059826	4.158583
301.353961	5896.906164	15.572071	-0.059802	4.155866
301.411623	5888.844593	15.577075	-0.059807	4.153137
301.280973	5880.857459	15.582080	-0.059778	4.150428
301.223961	5872.841740	15.587085	-0.059762	4.147710
301.412900	5864.855802	15.592090	-0.059792	4.145002
301.182881	5856.875985	15.597095	-0.059744	4.142290
301.129046	5848.858510	15.602099	-0.059729	4.139566
301.382264	5840.868454	15.607104	-0.059771	4.136852
301.381089	5832.857793	15.612109	-0.059765	4.134127
301.369965	5824.838112	15.617114	-0.059758	4.131397
301.282122	5816.843929	15.622119	-0.059737	4.128673
301.285445	5808.858157	15.627123	-0.059732	4.125951
301.220136	5800.900302	15.632128	-0.059715	4.123236
300.926637	5792.875651	15.637133	-0.059655	4.120493
300.941655	5784.924561	15.642138	-0.059652	4.117777
300.842048	5776.877965	15.647143	-0.059629	4.115026
300.697220	5768.824802	15.652147	-0.059596	4.112270
300.783186	5760.827711	15.657152	-0.059607	4.109534
300.674316	5752.830515	15.662157	-0.059582	4.106794
300.575957	5744.869274	15.667162	-0.059558	4.104064
300.651219	5736.853970	15.672167	-0.059567	4.101317
300.870688	5728.843034	15.677171	-0.059603	4.098570
300.860086	5720.868970	15.682176	-0.059596	4.095832
300.441978	5712.876971	15.687181	-0.059512	4.093080
300.615060	5704.855724	15.692186	-0.059539	4.090325
300.733890	5696.855546	15.697191	-0.059556	4.087574
300.585550	5688.877556	15.702195	-0.059524	4.084825
300.541623	5680.933491	15.707200	-0.059510	4.082087
300.538990	5672.898096	15.712205	-0.059505	4.079316
300.450345	5664.975626	15.717210	-0.059483	4.076582
300.369297	5656.873800	15.722215	-0.059463	4.073784
300.502124	5648.856595	15.727219	-0.059482	4.071016
300.317771	5640.898251	15.732224	-0.059443	4.068262
300.256936	5632.867287	15.737229	-0.059426	4.065483
300.437925	5624.899581	15.742234	-0.059454	4.062727
300.438536	5616.887861	15.747239	-0.059449	4.059951
300.197809	5608.935691	15.752243	-0.059399	4.057191
300.230906	5600.916519	15.757248	-0.059400	4.054410
300.270316	5592.889994	15.762253	-0.059402	4.051624
300.209675	5584.901015	15.767258	-0.059386	4.048848
300.017880	5576.935627	15.772263	-0.059345	4.046076
300.010582	5568.923138	15.777267	-0.059339	4.043289
300.214599	5560.933227	15.782272	-0.059371	4.040511
300.006732	5552.911623	15.787277	-0.059327	4.037713
299.942060	5544.906556	15.792282	-0.059310	4.034922
300.126732	5536.799720	15.797287	-0.059339	4.032097
299.994580	5528.792639	15.802291	-0.059309	4.029300
299.776278	5520.893197	15.807296	-0.059264	4.026537
299.617930	5512.855594	15.812301	-0.059229	4.023725
299.802987	5504.878252	15.817306	-0.059258	4.020937
299.653159	5496.913955	15.822311	-0.059225	4.018147
299.621264	5488.893032	15.827315	-0.059214	4.015337
299.641938	5480.882538	15.832320	-0.059213	4.012530
299.799261	5472.812844	15.837325	-0.059237	4.009701
299.715267	5464.908942	15.842330	-0.059216	4.006926
299.849774	5456.868364	15.847335	-0.059236	4.004103
299.780303	5448.924288	15.852339	-0.059218	4.001310
299.712202	5440.933388	15.857344	-0.059200	3.998498
299.577573	5432.937873	15.862349	-0.059169	3.995681
299.678624	5424.882363	15.867354	-0.059183	3.992845
299.345529	5416.883445	15.872359	-0.059116	3.990020
299.631241	5408.860945	15.877363	-0.059164	3.987195
299.515280	5400.868791	15.882368	-0.059137	3.984371
299.266567	5392.907961	15.887373	-0.059085	3.981555
299.113008	5384.871632	15.892378	-0.059052	3.978711
299.281298	5376.916905	15.897383	-0.059078	3.975900
299.241157	5368.886747	15.902387	-0.059065	3.973057
299.231219	5360.887362	15.907392	-0.059058	3.970222
299.317223	5352.894431	15.912397	-0.059069	3.967390
299.461906	5344.910543	15.917402	-0.059091	3.964560
299.136129	5336.968861	15.922407	-0.059025	3.961735
299.011164	5328.929359	15.927411	-0.058996	3.958876
299.407975	5320.961861	15.932416	-0.059065	3.956050
299.270368	5312.888925	15.937421	-0.059034	3.953176
299.077355	5304.897368	15.942426	-0.058993	3.950327
299.167516	5296.914492	15.947431	-0.059005	3.947484
299.009404	5288.921488	15.952435	-0.058970	3.944631
299.011971	5280.964921	15.957440	-0.058965	3.941792
298.849659	5272.944450	15.962445	-0.058930	3.938925
298.950194	5264.931714	15.967450	-0.058943	3.936063
298.752539	5256.926515	15.972455	-0.058901	3.933197
298.763684	5248.929022	15.977459	-0.058898	3.930335
298.857206	5240.988997	15.982464	-0.058910	3.927493
298.913362	5232.945978	15.987469	-0.058916	3.924612
298.710012	5225.018545	15.992474	-0.058873	3.921765
298.818485	5216.953331	15.997479	-0.058888	3.918872
298.832413	5208.969224	16.002483	-0.058885	3.916004
298.727176	5200.951909	16.007488	-0.058860	3.913120
298.647171	5192.911499	16.012493	-0.058840	3.910227
298.750211	5184.983825	16.017498	-0.058854	3.907375
298.461945	5176.968642	16.022503	-0.058795	3.904482
298.487757	5168.964876	16.027507	-0.058795	3.901597
298.646070	5160.956667	16.032512	-0.058819	3.898710
298.509804	5152.972317	16.037517	-0.058789	3.895825
298.367834	5144.948468	16.042522	-0.058757	3.892923
298.331302	5136.919941	16.047527	-0.058745	3.890019
298.411493	5128.978367	16.052531	-0.058755	3.887147
298.482892	5120.974159	16.057536	-0.058763	3.884250
298.343273	5112.989716	16.062541	-0.058731	3.881354
298.544727	5104.983611	16.067546	-0.058764	3.878454
298.314038	5096.970471	16.072551	-0.058716	3.875541
298.141506	5088.763577	16.077555	-0.058678	3.872557
298.182300	5080.783372	16.082560	-0.058681	3.869657
298.049355	5072.860594	16.087565	-0.058651	3.866772
298.060758	5064.931653	16.092570	-0.058648	3.863886
298.168656	5056.918565	16.097575	-0.058663	3.860969
298.158779	5048.931642	16.102579	-0.058655	3.858056
298.025952	5040.967784	16.107584	-0.058626	3.855148
297.879461	5032.940670	16.112589	-0.058593	3.852214
298.162175	5024.921600	16.117594	-0.058640	3.849289
297.942857	5016.967976	16.122599	-0.058594	3.846376
297.870499	5008.973060	16.127603	-0.058576	3.843449
297.738345	5001.011476	16.132608	-0.058546	3.840530
297.730113	4993.033725	16.137613	-0.058539	3.837605
298.006286	4984.982239	16.142618	-0.058585	3.834658
297.631329	4976.989788	16.147623	-0.058510	3.831716
297.653709	4968.986204	16.152627	-0.058509	3.828776
297.633833	4960.989471	16.157632	-0.058501	3.825835
297.561967	4953.011201	16.162637	-0.058482	3.822898
297.612641	4945.007501	16.167642	-0.058486	3.819952
297.555591	4937.055108	16.172647	-0.058470	3.817020
297.478078	4929.013573	16.177651	-0.058451	3.814052
297.499219	4920.997146	16.182656	-0.058449	3.811094
297.582980	4913.016254	16.187661	-0.058460	3.808148
297.404828	4905.023002	16.192666	-0.058421	3.805189
297.512122	4897.092751	16.197671	-0.058436	3.802257
297.390450	4889.040400	16.202675	-0.058408	3.799273
297.442335	4881.117294	16.207680	-0.058413	3.796339
297.340615	4873.038528	16.212685	-0.058389	3.793341
297.411702	4865.040894	16.217690	-0.058397	3.790374
297.343962	4857.021617	16.222695	-0.058379	3.787394
297.111357	4849.031950	16.227699	-0.058330	3.784419
297.333352	4841.077690	16.232704	-0.058367	3.781465
297.241320	4833.052836	16.237709	-0.058344	3.778476
297.037452	4825.071267	16.242714	-0.058301	3.775497
296.939845	4817.074609	16.247719	-0.058278	3.772513
296.898840	4809.036575	16.252723	-0.058265	3.769513
296.808097	4801.084864	16.257728	-0.058243	3.766541
296.845948	4793.062334	16.262733	-0.058245	3.763543
296.846575	4785.045960	16.267738	-0.058239	3.760544
296.936552	4777.085521	16.272743	-0.058251	3.757566
296.784616	4769.049631	16.277747	-0.058218	3.754552
296.961058	4761.064074	16.282752	-0.058245	3.751562
296.893384	4753.040891	16.287757	-0.058227	3.748549
296.853778	4745.044884	16.292762	-0.058215	3.745545
296.683804	4737.109937	16.297767	-0.058178	3.742559
296.538664	4729.056241	16.302771	-0.058146	3.739526
296.548735	4721.126240	16.307776	-0.058142	3.736541
296.377184	4713.095563	16.312781	-0.058105	3.733511
296.436419	4705.063543	16.317786	-0.058111	3.730483
296.372832	4697.100375	16.322791	-0.058094	3.727476
296.325871	4689.087252	16.327795	-0.058080	3.724449
296.440044	4681.167828	16.332800	-0.058096	3.721458
296.441916	4673.117542	16.337805	-0.058091	3.718412
296.511824	4665.165108	16.342810	-0.058099	3.715403
296.296267	4657.087551	16.347815	-0.058054	3.712337
296.319021	4649.029385	16.352819	-0.058053	3.709281
296.360318	4641.092585	16.357824	-0.058055	3.706270
296.349083	4633.074442	16.362829	-0.058048	3.703224
296.468212	4625.108604	16.367834	-0.058065	3.700198
296.357410	4617.161773	16.372839	-0.058039	3.697172
296.206183	4609.147935	16.377843	-0.058006	3.694116
295.974743	4601.169810	16.382848	-0.057958	3.691070
296.153692	4593.126374	16.387853	-0.057986	3.688006
296.086924	4585.166260	16.392858	-0.057968	3.684966
295.806130	4577.239170	16.397863	-0.057911	3.681930
295.917478	4569.176011	16.402867	-0.057926	3.678849
296.014824	4561.198774	16.407872	-0.057939	3.675799
295.850773	4553.188547	16.412877	-0.057903	3.672726
295.884414	4545.171047	16.417882	-0.057904	3.669654
295.771571	4537.223775	16.422887	-0.057878	3.666602
295.763330	4529.181045	16.427891	-0.057871	3.663513
295.751665	4521.203804	16.432896	-0.057864	3.660447
295.483545	4513.233593	16.437901	-0.057809	3.657374
295.648917	4505.192116	16.442906	-0.057834	3.654283
295.631702	4497.190875	16.447911	-0.057826	3.651200
295.538994	4489.186998	16.452915	-0.057804	3.648111
295.513721	4481.220095	16.457920	-0.057794	3.645035
295.508292	4473.242412	16.462925	-0.057787	3.641954
295.414566	4465.259815	16.467930	-0.057765	3.638865
295.411512	4457.247130	16.472935	-0.057759	3.635764
295.264262	4449.197290	16.477939	-0.057726	3.632643
295.289974	4441.222129	16.482944	-0.057726	3.629553
295.461024	4433.205015	16.487949	-0.057753	3.626447
295.511772	4425.210338	16.492954	-0.057757	3.623344
295.333887	4417.252966	16.497959	-0.057719	3.620247
295.131208	4409.260902	16.502963	-0.057676	3.617134
295.262466	4401.280349	16.507968	-0.057695	3.614031
295.044397	4393.254381	16.512973	-0.057649	3.610898
295.094673	4385.282096	16.517978	-0.057653	3.607790
295.209288	4377.258520	16.522983	-0.057669	3.604662
295.031091	4369.315447	16.527987	-0.057631	3.601554
295.000302	4361.315307	16.532992	-0.057620	3.598426
294.932105	4353.314455	16.537997	-0.057602	3.595293
295.052379	4345.283175	16.543002	-0.057619	3.592151
295.035870	4337.312509	16.548007	-0.057611	3.589027
294.953051	4329.342448	16.553011	-0.057590	3.585897
294.969737	4321.356290	16.558016	-0.057588	3.582762
294.918051	4313.338412	16.563021	-0.057574	3.579609
294.956603	4305.377386	16.568026	-0.057576	3.576479
294.847698	4297.360363	16.573031	-0.057550	3.573319
294.700463	4289.328740	16.578035	-0.057517	3.570150
294.520107	4281.396158	16.583040	-0.057479	3.567016
294.579004	4273.355804	16.588045	-0.057484	3.563844
294.563675	4265.399935	16.593050	-0.057476	3.560700
294.497273	4257.424894	16.598055	-0.057459	3.557545
294.492009	4249.362553	16.603059	-0.057453	3.554353
294.600844	4241.284016	16.608064	-0.057468	3.551156
294.407623	4233.306834	16.613069	-0.057426	3.547987
294.301389	4225.335092	16.618074	-0.057402	3.544820
294.274012	4217.392901	16.623079	-0.057391	3.541664
294.226134	4209.380073	16.628083	-0.057377	3.538477
294.363482	4201.380935	16.633088	-0.057397	3.535298
294.284736	4193.384877	16.638093	-0.057378	3.532111
294.381999	4185.378844	16.643098	-0.057391	3.528922
294.335185	4177.398760	16.648103	-0.057377	3.525736
294.178874	4169.430338	16.653107	-0.057342	3.522549
294.289264	4161.423886	16.658112	-0.057358	3.519352
294.102692	4153.470765	16.663117	-0.057318	3.516164
293.963196	4145.466016	16.668122	-0.057287	3.512954
294.043944	4137.433045	16.673127	-0.057296	3.509736
294.023933	4129.429949	16.678131	-0.057287	3.506525
294.103889	4121.458339	16.683136	-0.057297	3.503326
294.066243	4113.471253	16.688141	-0.057285	3.500114
294.018342	4105.502399	16.693146	-0.057271	3.496907
293.879667	4097.487502	16.698151	-0.057240	3.493675
293.907074	4089.454750	16.703155	-0.057240	3.490438
294.048416	4081.504843	16.708160	-0.057261	3.487235
293.970040	4073.492852	16.713165	-0.057241	3.483997
293.702374	4065.572708	16.718170	-0.057186	3.480788
293.681703	4057.585776	16.723175	-0.057177	3.477556
293.695307	4049.529600	16.728179	-0.057174	3.474294
293.658052	4041.550454	16.733184	-0.057162	3.471059
293.473489	4033.525080	16.738189	-0.057123	3.467797
293.456241	4025.540913	16.743194	-0.057114	3.464554
293.424282	4017.590742	16.748199	-0.057103	3.461321
293.455534	4009.544790	16.753203	-0.057104	3.458049
293.601759	4001.576925	16.758208	-0.057126	3.454809
293.401981	3993.564644	16.763213	-0.057083	3.451536
293.380098	3985.564857	16.768218	-0.057074	3.448272
293.447786	3977.595234	16.773223	-0.057081	3.445019
293.489611	3969.619935	16.778227	-0.057084	3.441760
293.392077	3961.639833	16.783232	-0.057061	3.438492
293.207377	3953.638643	16.788237	-0.057021	3.435209
293.306949	3945.601480	16.793242	-0.057034	3.431917
293.391105	3937.605185	16.798247	-0.057045	3.428639
293.234258	3929.602805	16.803251	-0.057010	3.425347
293.328495	3921.637687	16.808256	-0.057023	3.422075
293.119687	3913.675499	16.813261	-0.056979	3.418791
293.006473	3905.669245	16.818266	-0.056952	3.415490
293.107795	3897.686362	16.823271	-0.056966	3.412202
292.887749	3889.678776	16.828275	-0.056920	3.408889
293.006992	3881.665263	16.833280	-0.056937	3.405583
293.029450	3873.706776	16.838285	-0.056936	3.402292
292.962037	3865.706184	16.843290	-0.056918	3.398978
292.979975	3857.736420	16.848295	-0.056916	3.395677
292.921160	3849.667224	16.853299	-0.056900	3.392328
292.766651	3841.677955	16.858304	-0.056866	3.389006
292.705632	3833.706749	16.863309	-0.056850	3.385691
292.611410	3825.731180	16.868314	-0.056827	3.382371
292.736337	3817.762946	16.873319	-0.056845	3.379057
292.920838	3809.757743	16.878323	-0.056874	3.375727
292.742602	3801.788182	16.883328	-0.056836	3.372396
292.436371	3793.785924	16.888333	-0.056774	3.369043
292.438161	3785.796845	16.893338	-0.056769	3.365704
292.440195	3777.820152	16.898343	-0.056764	3.362366
292.190731	3769.819306	16.903347	-0.056712	3.359006
292.263133	3761.842843	16.908352	-0.056720	3.355664
292.244051	3753.813773	16.913357	-0.056712	3.352293
292.248416	3745.784825	16.918362	-0.056707	3.348920
292.327985	3737.819049	16.923367	-0.056717	3.345573
292.324135	3729.839535	16.928371	-0.056711	3.342214
292.457637	3721.853894	16.933376	-0.056731	3.338854
292.087136	3713.875738	16.938381	-0.056657	3.335475
292.163106	3705.845449	16.943386	-0.056665	3.332087
292.033088	3697.879702	16.948391	-0.056636	3.328715
292.094869	3689.883891	16.953395	-0.056642	3.325334
291.978426	3681.954576	16.958400	-0.056616	3.321972
291.945948	3673.935429	16.963405	-0.056604	3.318571
292.020369	3665.913620	16.968410	-0.056613	3.315169
292.009955	3657.915594	16.973415	-0.056606	3.311770
291.851692	3649.905873	16.978419	-0.056571	3.308358
291.773281	3641.941381	16.983424	-0.056551	3.304965
291.784282	3633.985206	16.988429	-0.056548	3.301574
291.689800	3625.993947	16.993434	-0.056525	3.298162
291.898230	3617.978083	16.998439	-0.056559	3.294747
291.788498	3609.995289	17.003443	-0.056533	3.291330
291.610897	3602.024019	17.008448	-0.056495	3.287912
291.684083	3593.988300	17.013453	-0.056503	3.284472
291.534221	3586.056029	17.018458	-0.056470	3.281065
291.603605	3578.058471	17.023463	-0.056478	3.277635
291.520314	3570.051132	17.028467	-0.056457	3.274190
291.669206	3562.039897	17.033472	-0.056480	3.270750
291.532497	3554.047056	17.038477	-0.056449	3.267303
291.568376	3546.056400	17.043482	-0.056451	3.263859
291.522458	3538.104773	17.048487	-0.056437	3.260426
291.237991	3530.127041	17.053491	-0.056379	3.256968
291.500364	3522.118588	17.058496	-0.056423	3.253515
291.377283	3514.079704	17.063501	-0.056394	3.250030
291.428534	3506.113369	17.068506	-0.056399	3.246580
291.269717	3498.164801	17.073511	-0.056364	3.243125
291.185333	3490.162577	17.078515	-0.056343	3.239646
291.237608	3482.202978	17.083520	-0.056348	3.236188
291.132010	3474.146804	17.088525	-0.056323	3.232677
291.002072	3466.143238	17.093530	-0.056293	3.229184
291.135185	3458.126726	17.098535	-0.056313	3.225693
291.049893	3450.152106	17.103539	-0.056292	3.222207
291.057919	3442.207400	17.108544	-0.056288	3.218735
290.945070	3434.224143	17.113549	-0.056262	3.215237
290.956877	3426.202298	17.118554	-0.056259	3.211723
290.949487	3418.230881	17.123559	-0.056252	3.208226
290.748896	3410.233812	17.128563	-0.056210	3.204707
290.952292	3402.279107	17.133568	-0.056243	3.201219
290.711512	3394.334667	17.138573	-0.056193	3.197713
290.551244	3386.329077	17.143578	-0.056157	3.194180
290.563947	3378.283412	17.148583	-0.056155	3.190633
290.700414	3370.281534	17.153587	-0.056175	3.187106
290.657450	3362.331722	17.158592	-0.056162	3.183590
290.549242	3354.339842	17.163597	-0.056136	3.180050
290.529029	3346.342135	17.168602	-0.056127	3.176506
290.558066	3338.367628	17.173607	-0.056128	3.172971
290.504226	3330.329154	17.178611	-0.056112	3.169400
290.698373	3322.367094	17.183616	-0.056143	3.165870
290.553020	3314.411603	17.188621	-0.056111	3.162324
290.503672	3306.414476	17.193626	-0.056097	3.158760
290.344621	3298.450351	17.198631	-0.056062	3.155201
290.362694	3290.404672	17.203635	-0.056060	3.151610
290.224466	3282.434360	17.208640	-0.056029	3.148041
290.135679	3274.440434	17.213645	-0.056007	3.144460
290.061871	3266.477876	17.218650	-0.055988	3.140890
289.952662	3258.532755	17.223655	-0.055963	3.137322
290.011232	3250.488509	17.228659	-0.055969	3.133713
290.153283	3242.493178	17.233664	-0.055990	3.130125
290.005661	3234.527209	17.238669	-0.055957	3.126533
289.803149	3226.547503	17.243674	-0.055914	3.122929
289.770042	3218.565867	17.248679	-0.055903	3.119327
289.705261	3210.606976	17.253683	-0.055886	3.115730
289.730292	3202.579369	17.258688	-0.055885	3.112102
289.973740	3194.566234	17.263693	-0.055925	3.108485
289.881015	3186.566948	17.268698	-0.055903	3.104856
289.774467	3178.654783	17.273703	-0.055878	3.101261
289.778850	3170.643189	17.278707	-0.055873	3.097622
289.890578	3162.636407	17.283712	-0.055889	3.093986
289.774848	3154.652958	17.288717	-0.055862	3.090346
289.567634	3146.699149	17.293722	-0.055818	3.086711
289.641369	3138.708670	17.298727	-0.055827	3.083067
289.768489	3130.690104	17.303731	-0.055845	3.079409
289.588664	3122.763276	17.308736	-0.055807	3.075775
289.256622	3114.702646	17.313741	-0.055740	3.072067
289.558488	3106.653407	17.318746	-0.055791	3.068390
289.596572	3098.699004	17.323751	-0.055793	3.064740
289.436110	3090.748550	17.328755	-0.055758	3.061078
289.516524	3082.773550	17.333760	-0.055767	3.057411
289.498196	3074.798565	17.338765	-0.055759	3.053736
289.272292	3066.803116	17.343770	-0.055711	3.050036
289.130352	3058.852751	17.348775	-0.055680	3.046357
289.336836	3050.824186	17.353779	-0.055713	3.042654
289.301700	3042.868663	17.358784	-0.055701	3.038969
289.167391	3034.901441	17.363789	-0.055671	3.035269
289.196859	3026.886016	17.368794	-0.055671	3.031550
289.301146	3018.901511	17.373799	-0.055686	3.027845
288.901772	3010.924164	17.378803	-0.055606	3.024114
288.914413	3002.970835	17.383808	-0.055603	3.020409
289.068706	2994.988379	17.388813	-0.055627	3.016693
288.970147	2986.979345	17.393818	-0.055603	3.012948
288.955405	2978.990216	17.398823	-0.055595	3.009212
288.881771	2970.993214	17.403827	-0.055576	3.005464
288.732112	2963.070137	17.408832	-0.055543	3.001743
288.650688	2955.083294	17.413837	-0.055523	2.997990
288.716174	2947.061764	17.418842	-0.055530	2.994224
288.886493	2939.043844	17.423847	-0.055557	2.990460
288.816268	2931.053486	17.428851	-0.055538	2.986692
288.834495	2923.090973	17.433856	-0.055536	2.982936
288.903748	2915.108608	17.438861	-0.055544	2.979170
288.698698	2907.150367	17.443866	-0.055501	2.975396
288.666879	2899.160113	17.448871	-0.055490	2.971611
288.623203	2891.151713	17.453875	-0.055476	2.967812
288.604633	2883.193621	17.458880	-0.055468	2.964033
288.547229	2875.230166	17.463885	-0.055452	2.960245
288.405839	2867.264992	17.468890	-0.055420	2.956446
288.526362	2859.260304	17.473895	-0.055438	2.952638
288.316887	2851.256388	17.478899	-0.055393	2.948808
288.284611	2843.277123	17.483904	-0.055382	2.944994
288.258690	2835.323176	17.488909	-0.055372	2.941187
288.254565	2827.332236	17.493914	-0.055366	2.937359
288.235180	2819.359880	17.498919	-0.055357	2.933534
288.316052	2811.313611	17.503923	-0.055367	2.929673
288.329199	2803.365738	17.508928	-0.055365	2.925852
287.908038	2795.445258	17.513933	-0.055281	2.922015
288.039056	2787.428362	17.518938	-0.055300	2.918156
288.110440	2779.443404	17.523943	-0.055308	2.914305
287.896590	2771.379631	17.528947	-0.055263	2.910395
287.959890	2763.398770	17.533952	-0.055270	2.906535
288.029743	2755.424540	17.538957	-0.055278	2.902673
287.851746	2747.476691	17.543962	-0.055239	2.898805
287.728810	2739.523824	17.548967	-0.055211	2.894933
287.620350	2731.536471	17.553971	-0.055186	2.891039
287.692152	2723.544403	17.558976	-0.055194	2.887148
287.603808	2715.580884	17.563981	-0.055172	2.883257
287.408154	2707.595430	17.568986	-0.055131	2.879344
287.614429	2699.656409	17.573991	-0.055164	2.875470
287.495641	2691.618518	17.578995	-0.055137	2.871525
287.408783	2683.649836	17.584000	-0.055115	2.867610
287.458014	2675.669196	17.589005	-0.055119	2.863691
287.496635	2667.680989	17.594010	-0.055121	2.859763
287.633040	2659.719325	17.599015	-0.055141	2.855847
287.334792	2651.741641	17.604019	-0.055081	2.851894
287.550227	2643.745569	17.609024	-0.055116	2.847956
287.403897	2635.754715	17.614029	-0.055083	2.843994
287.349614	2627.798015	17.619034	-0.055068	2.840049
287.318759	2619.861687	17.624039	-0.055057	2.836109
287.162592	2611.844536	17.629043	-0.055023	2.832117
287.021485	2603.873425	17.634048	-0.054991	2.828143
287.091516	2595.870716	17.639053	-0.054999	2.824160
287.050184	2587.896366	17.644058	-0.054986	2.820179
287.075039	2579.933837	17.649063	-0.054986	2.816202
286.755810	2571.955293	17.654067	-0.054921	2.812191
286.797456	2563.963654	17.659072	-0.054924	2.808189
286.742069	2555.985226	17.664077	-0.054908	2.804182
286.667106	2548.031042	17.669082	-0.054889	2.800181
286.659882	2540.087265	17.674087	-0.054882	2.796183
286.635033	2532.051654	17.679091	-0.054873	2.792132
286.610072	2524.055548	17.684096	-0.054863	2.788094
286.674699	2516.069898	17.689101	-0.054870	2.784062
286.679903	2508.108235	17.694106	-0.054865	2.780033
286.716239	2500.174182	17.699111	-0.054867	2.776013
286.521531	2492.172840	17.704115	-0.054826	2.771940
286.717482	2484.174550	17.709120	-0.054857	2.767885
286.636585	2476.209233	17.714125	-0.054837	2.763825
286.468109	2468.273272	17.719130	-0.054800	2.759769
286.524497	2460.306178	17.724135	-0.054805	2.755704
286.286285	2452.256729	17.729139	-0.054756	2.751573
286.107066	2444.291128	17.734144	-0.054717	2.747483
286.240891	2436.295692	17.739149	-0.054737	2.743390
286.365193	2428.311414	17.744154	-0.054755	2.739296
286.294346	2420.379078	17.749159	-0.054737	2.735211
286.004586	2412.386495	17.754163	-0.054677	2.731075
286.177651	2404.407446	17.759168	-0.054704	2.726968
286.100182	2396.450799	17.764173	-0.054685	2.722851
285.835576	2388.502000	17.769178	-0.054630	2.718721
285.935764	2380.528519	17.774183	-0.054644	2.714594
285.888497	2372.513222	17.779187	-0.054630	2.710430
285.758962	2364.551914	17.784192	-0.054601	2.706282
285.799972	2356.584829	17.789197	-0.054603	2.702136
285.786593	2348.617938	17.794202	-0.054595	2.697980
285.929076	2340.633829	17.799207	-0.054617	2.693818
285.653609	2332.652105	17.804211	-0.054560	2.689625
285.648571	2324.697383	17.809216	-0.054554	2.685457
285.582399	2316.739219	17.814221	-0.054537	2.681276
285.309474	2308.801914	17.819226	-0.054481	2.677087
285.314157	2300.802048	17.824231	-0.054476	2.672875
285.387126	2292.775727	17.829235	-0.054485	2.668648
285.468604	2284.803574	17.834240	-0.054495	2.664443
285.296889	2276.864777	17.839245	-0.054457	2.660233
285.587342	2268.850453	17.844250	-0.054506	2.656005
285.415038	2260.907625	17.849255	-0.054469	2.651779
285.201659	2252.933868	17.854259	-0.054424	2.647528
285.489298	2244.945016	17.859264	-0.054473	2.643293
285.559147	2236.994368	17.864269	-0.054480	2.639059
285.397772	2229.035517	17.869274	-0.054445	2.634798
285.507067	2221.042295	17.874279	-0.054460	2.630529
285.219445	2213.075433	17.879283	-0.054402	2.626242
285.117375	2205.133695	17.884288	-0.054377	2.621973
285.155154	2197.169070	17.889293	-0.054379	2.617694
285.070948	2189.183605	17.894298	-0.054358	2.613389
285.066497	2181.188430	17.899303	-0.054352	2.609076
284.918041	2173.228708	17.904307	-0.054319	2.604766
285.277152	2165.253627	17.909312	-0.054381	2.600475
285.038052	2157.323225	17.914317	-0.054331	2.596161
284.779924	2149.230407	17.919322	-0.054278	2.591750
284.939730	2141.192436	17.924327	-0.054303	2.587389
284.712925	2133.267036	17.929331	-0.054255	2.583056
284.776382	2125.331214	17.934336	-0.054262	2.578730
284.919338	2117.369285	17.939341	-0.054283	2.574388
284.834294	2109.391001	17.944346	-0.054262	2.570014
284.741052	2101.479705	17.949351	-0.054240	2.565669
284.603659	2093.517883	17.954355	-0.054209	2.561285
284.355863	2085.594217	17.959360	-0.054158	2.556907
284.400139	2077.607383	17.964365	-0.054161	2.552507
284.269530	2069.615801	17.969370	-0.054131	2.548085
284.607762	2061.625691	17.974375	-0.054189	2.543689
284.449812	2053.691204	17.979379	-0.054155	2.539281
284.517869	2045.721276	17.984384	-0.054162	2.534861
284.299916	2037.766921	17.989389	-0.054116	2.530423
284.189685	2029.791605	17.994394	-0.054091	2.525972
284.230034	2021.856129	17.999399	-0.054093	2.521547
284.173036	2013.889002	18.004403	-0.054077	2.517089
283.988675	2005.918116	18.009408	-0.054038	2.512612
284.076143	1997.903798	18.014413	-0.054049	2.508122
283.844417	1989.954862	18.019418	-0.054000	2.503638
284.126984	1981.977803	18.024423	-0.054048	2.499167
284.023907	1974.024553	18.029427	-0.054023	2.494673
283.943085	1966.067631	18.034432	-0.054003	2.490171
283.901426	1958.096927	18.039437	-0.053990	2.485656
283.742494	1950.166114	18.044442	-0.053956	2.481146
283.832276	1942.201577	18.049447	-0.053967	2.476628
283.657073	1934.233931	18.054451	-0.053929	2.472080
283.665659	1926.241513	18.059456	-0.053926	2.467523
283.714328	1918.286734	18.064461	-0.053930	2.462982
283.667149	1910.321240	18.069466	-0.053916	2.458419
283.699775	1902.384044	18.074471	-0.053916	2.453870
283.371808	1894.431979	18.079475	-0.053850	2.449277
283.564254	1886.424547	18.084480	-0.053881	2.444683
283.482187	1878.516537	18.089485	-0.053860	2.440116
283.469219	1870.537075	18.094490	-0.053853	2.435505
283.486873	1862.513725	18.099495	-0.053851	2.430863
283.258061	1854.548178	18.104499	-0.053803	2.426225
283.283282	1846.601175	18.109504	-0.053803	2.421610
283.402874	1838.645016	18.114509	-0.053820	2.416987
283.257918	1830.680791	18.119514	-0.053788	2.412331
283.189405	1822.740288	18.124519	-0.053770	2.407685
283.220272	1814.766774	18.129523	-0.053770	2.403018
283.182861	1806.824725	18.134528	-0.053758	2.398356
283.102547	1798.887409	18.139533	-0.053738	2.393684
283.142322	1790.876514	18.144538	-0.053740	2.388969
283.122386	1782.926646	18.149543	-0.053731	2.384275
283.044628	1774.992533	18.154547	-0.053712	2.379578
283.020284	1767.044853	18.159552	-0.053702	2.374867
282.972182	1759.080941	18.164557	-0.053688	2.370135
282.686403	1751.133736	18.169562	-0.053629	2.365385
282.603927	1743.215309	18.174567	-0.053609	2.360659
282.614584	1735.252438	18.179571	-0.053606	2.355904
282.593426	1727.255204	18.184576	-0.053597	2.351116
282.560447	1719.289645	18.189581	-0.053585	2.346336
282.519948	1711.331485	18.194586	-0.053573	2.341551
282.595098	1703.385830	18.199591	-0.053581	2.336773
282.391049	1695.426077	18.204595	-0.053538	2.331953
282.327093	1687.478282	18.209600	-0.053521	2.327143
282.475729	1679.517726	18.214605	-0.053544	2.322332
282.158994	1671.612405	18.219610	-0.053479	2.317506
282.401651	1663.623469	18.224615	-0.053519	2.312666
282.370027	1655.637211	18.229619	-0.053508	2.307794
282.249628	1647.715213	18.234624	-0.053481	2.302944
282.008639	1639.808184	18.239629	-0.053431	2.298082
281.973967	1631.831994	18.244634	-0.053419	2.293185
282.091856	1623.861240	18.249639	-0.053436	2.288294
282.057909	1615.902548	18.254643	-0.053424	2.283387
281.901093	1607.988537	18.259648	-0.053390	2.278487
281.899567	1600.018532	18.264653	-0.053385	2.273554
281.984763	1591.979392	18.269658	-0.053395	2.268576
281.854209	1584.054705	18.274663	-0.053366	2.263639
281.887297	1576.105401	18.279667	-0.053367	2.258690
281.658939	1568.189583	18.284672	-0.053319	2.253728
281.585676	1560.236365	18.289677	-0.053300	2.248746
281.435832	1552.291340	18.294682	-0.053267	2.243750
281.595652	1544.354133	18.299687	-0.053292	2.238776
281.296431	1536.430014	18.304691	-0.053231	2.233758
281.342899	1528.445142	18.309696	-0.053234	2.228722
281.487057	1520.476661	18.314701	-0.053256	2.223693
281.556712	1512.529168	18.319706	-0.053264	2.218659
281.619061	1504.602882	18.324711	-0.053270	2.213627
281.578110	1496.639339	18.329715	-0.053257	2.208550
281.382402	1488.736680	18.334720	-0.053216	2.203486
281.246883	1480.830905	18.339725	-0.053186	2.198414
281.057078	1472.873344	18.344730	-0.053145	2.193293
281.176439	1464.878631	18.349735	-0.053162	2.188163
281.098739	1456.943057	18.354739	-0.053142	2.183041
280.848193	1449.034249	18.359744	-0.053091	2.177909
280.921678	1441.077515	18.364749	-0.053099	2.172764
280.947238	1433.100976	18.369754	-0.053099	2.167589
280.922519	1425.185598	18.374759	-0.053089	2.162436
280.897513	1417.239640	18.379763	-0.053079	2.157252
280.988528	1409.282145	18.384768	-0.053091	2.152058
281.083714	1401.330570	18.389773	-0.053103	2.146856
280.666795	1393.433298	18.394778	-0.053021	2.141629
280.751195	1385.501944	18.399783	-0.053031	2.136414
280.629598	1377.555685	18.404787	-0.053003	2.131157
280.650903	1369.611859	18.409792	-0.053002	2.125901
280.714166	1361.679251	18.414797	-0.053009	2.120645
280.642225	1353.752447	18.419802	-0.052990	2.115366
280.664972	1345.748553	18.424807	-0.052989	2.110031
280.497725	1337.805851	18.429811	-0.052953	2.104706
280.497313	1329.899225	18.434816	-0.052948	2.099408
280.526990	1321.973835	18.439821	-0.052948	2.094086
280.297317	1314.037206	18.444826	-0.052900	2.088718
280.331647	1306.114632	18.449831	-0.052901	2.083371
280.372457	1298.182162	18.454835	-0.052904	2.078005
280.255569	1290.245331	18.459840	-0.052877	2.072606
280.246836	1282.305911	18.464845	-0.052870	2.067202
280.207138	1274.373482	18.469850	-0.052858	2.061785
280.053059	1266.493446	18.474855	-0.052824	2.056379
280.007750	1258.539891	18.479859	-0.052810	2.050919
279.986971	1250.598944	18.484864	-0.052801	2.045455
280.164356	1242.665709	18.489869	-0.052829	2.040002
279.640868	1234.819143	18.494874	-0.052726	2.034524
279.947521	1226.801738	18.499879	-0.052778	2.028996
279.924744	1218.870396	18.504883	-0.052769	2.023480
279.656905	1210.977168	18.509888	-0.052714	2.017949
279.637909	1203.058282	18.514893	-0.052705	2.012412
279.567371	1195.112326	18.519898	-0.052687	2.006834
279.602874	1187.199165	18.524903	-0.052688	2.001276
279.420159	1179.296746	18.529907	-0.052649	1.995686
279.369728	1171.347097	18.534912	-0.052635	1.990062
279.693991	1163.380913	18.539917	-0.052690	1.984449
279.362558	1155.505914	18.544922	-0.052623	1.978815
279.391589	1147.592826	18.549927	-0.052623	1.973177
279.298570	1139.662755	18.554931	-0.052601	1.967497
279.282677	1131.755619	18.559936	-0.052593	1.961826
279.025191	1123.891026	18.564941	-0.052540	1.956143
279.048068	1115.895063	18.569946	-0.052539	1.950378
279.320526	1107.924446	18.574951	-0.052584	1.944642
279.096232	1100.052603	18.579955	-0.052537	1.938907
279.064390	1092.128765	18.584960	-0.052526	1.933137
278.963503	1084.223603	18.589965	-0.052502	1.927357
278.910798	1076.302364	18.594970	-0.052487	1.921552
279.010311	1068.409463	18.599975	-0.052501	1.915768
278.810954	1060.486440	18.604979	-0.052459	1.909911
278.859554	1052.558749	18.609984	-0.052462	1.904060
278.873366	1044.660206	18.614989	-0.052460	1.898208
278.744074	1036.756743	18.619994	-0.052431	1.892319
278.579893	1028.873440	18.624999	-0.052395	1.886422
278.653527	1020.941608	18.630003	-0.052404	1.880498
278.534002	1013.062030	18.635008	-0.052376	1.874572
278.450507	1005.135269	18.640013	-0.052355	1.868595
278.435398	997.213755	18.645018	-0.052347	1.862612
278.228326	989.346622	18.650023	-0.052304	1.856628
278.227428	981.421747	18.655027	-0.052298	1.850604
278.191828	973.508745	18.660032	-0.052287	1.844566
278.087835	965.637645	18.665037	-0.052262	1.838533
277.988003	957.730275	18.670042	-0.052238	1.832452
278.299515	949.769297	18.675047	-0.052291	1.826358
278.041745	941.911003	18.680051	-0.052238	1.820255
277.854071	934.048336	18.685056	-0.052198	1.814137
278.045687	926.113461	18.690061	-0.052229	1.807988
278.016207	918.218601	18.695066	-0.052218	1.801822
277.994714	910.354486	18.700071	-0.052209	1.795660
278.021686	902.378571	18.705075	-0.052209	1.789394
277.786462	894.508369	18.710080	-0.052160	1.783158
277.735231	886.644949	18.715085	-0.052145	1.776928
277.512636	878.759459	18.720090	-0.052099	1.770637
277.552542	870.868288	18.725095	-0.052101	1.764352
277.530169	862.993635	18.730099	-0.052092	1.758050
277.466215	855.104969	18.735104	-0.052075	1.751709
277.391849	847.220015	18.740109	-0.052056	1.745346
277.205929	839.365117	18.745114	-0.052016	1.738971
277.310551	831.464426	18.750119	-0.052030	1.732571
277.441383	823.545818	18.755123	-0.052049	1.726137
277.339314	815.693730	18.760128	-0.052025	1.719703
277.460626	807.807643	18.765133	-0.052043	1.713246
277.252377	799.925310	18.770138	-0.051999	1.706724
277.339635	792.045671	18.775143	-0.052010	1.700219
277.024314	784.222841	18.780147	-0.051946	1.693682
276.934524	776.335739	18.785152	-0.051924	1.687097
276.825028	768.487238	18.790157	-0.051899	1.680515
276.863227	760.612188	18.795162	-0.051901	1.673905
276.952391	752.712032	18.800167	-0.051912	1.667254
276.610707	744.891272	18.805171	-0.051844	1.660586
276.597078	737.026028	18.810176	-0.051836	1.653897
276.634108	729.133203	18.815181	-0.051838	1.647165
276.483924	721.292760	18.820186	-0.051805	1.640424
276.476069	713.439471	18.825191	-0.051798	1.633664
276.492177	705.506114	18.830195	-0.051796	1.626810
276.303367	697.683584	18.835200	-0.051756	1.619995
276.363526	689.829197	18.840205	-0.051762	1.613157
276.326519	681.951308	18.845210	-0.051750	1.606257
276.186574	674.142375	18.850215	-0.051719	1.599373
276.213707	666.285234	18.855219	-0.051719	1.592440
276.192434	658.418004	18.860224	-0.051709	1.585461
276.103924	650.599344	18.865229	-0.051688	1.578484
276.091430	642.746423	18.870234	-0.051680	1.571457
276.249757	634.876359	18.875239	-0.051705	1.564408
276.157850	627.070074	18.880243	-0.051683	1.557348
275.914764	619.245365	18.885248	-0.051632	1.550217
275.871879	611.415341	18.890253	-0.051619	1.543078
275.647711	603.604993	18.895258	-0.051572	1.535896
275.761713	595.749134	18.900263	-0.051588	1.528690
275.756120	587.915676	18.905267	-0.051582	1.521452
275.506851	580.136111	18.910272	-0.051531	1.514192
275.615973	572.274687	18.915277	-0.051546	1.506876
275.512308	564.459375	18.920282	-0.051522	1.499534
275.443156	556.656555	18.925287	-0.051504	1.492174
275.409299	548.836768	18.930291	-0.051492	1.484766
275.317768	541.050174	18.935296	-0.051470	1.477344
275.379967	533.182087	18.940301	-0.051477	1.469831
275.396320	525.350886	18.945306	-0.051475	1.462307
275.219246	517.588434	18.950311	-0.051437	1.454780
274.871064	509.820510	18.955315	-0.051367	1.447181
274.881239	502.017930	18.960320	-0.051364	1.439565
275.109090	494.186983	18.965325	-0.051401	1.431917
274.866551	486.415817	18.970330	-0.051351	1.424210
274.842506	478.636983	18.975335	-0.051341	1.416489
274.843727	470.832775	18.980339	-0.051336	1.408705
274.776403	463.061210	18.985344	-0.051319	1.400898
274.750317	455.296920	18.990349	-0.051309	1.393063
274.702379	447.495605	18.995354	-0.051295	1.385141
274.590769	439.749895	19.000359	-0.051269	1.377220
274.489411	431.979252	19.005363	-0.051245	1.369229
274.412017	424.218010	19.010368	-0.051226	1.361206
274.573182	416.442769	19.015373	-0.051251	1.353161
274.231689	408.717326	19.020378	-0.051182	1.345032
274.224428	400.963708	19.025383	-0.051176	1.336884
274.376085	393.172782	19.030387	-0.051199	1.328673
274.281980	385.448078	19.035392	-0.051176	1.320439
274.117593	377.683612	19.040397	-0.051141	1.312098
274.100721	369.854137	19.045402	-0.051132	1.303659
273.890497	362.176450	19.050407	-0.051088	1.295295
273.718238	354.468186	19.055411	-0.051051	1.286851
273.742215	346.749146	19.060416	-0.051051	1.278375
273.789181	339.026429	19.065421	-0.051054	1.269843
273.637170	331.326302	19.070426	-0.051021	1.261240
273.723292	323.614286	19.075431	-0.051032	1.252611
273.665393	315.919387	19.080435	-0.051016	1.243913
273.497748	308.255063	19.085440	-0.050980	1.235168
273.640806	300.518347	19.090445	-0.051002	1.226338
273.521014	292.849722	19.095450	-0.050974	1.217471
273.333456	285.200872	19.100455	-0.050934	1.208548
273.191812	277.555140	19.105459	-0.050903	1.199572
273.300708	269.855916	19.110464	-0.050918	1.190515
273.400504	262.181414	19.115469	-0.050932	1.181416
273.175396	254.564739	19.120474	-0.050885	1.172250
273.154631	246.926864	19.125479	-0.050876	1.163028
273.177744	239.282548	19.130483	-0.050875	1.153734
272.881287	231.654122	19.135488	-0.050815	1.144316
272.830100	224.047709	19.140493	-0.050801	1.134899
272.670994	216.436190	19.145498	-0.050766	1.125375
272.653305	208.839914	19.150503	-0.050758	1.115818
272.648674	201.225708	19.155507	-0.050752	1.106159
272.578028	193.647363	19.160512	-0.050734	1.096447
272.609369	186.054917	19.165517	-0.050735	1.086652
272.326188	178.533115	19.170522	-0.050677	1.076789
272.268076	170.959201	19.175527	-0.050662	1.066818
272.433771	163.379069	19.180531	-0.050688	1.056796
272.226061	155.859203	19.185536	-0.050644	1.046672
272.191356	148.349164	19.190541	-0.050633	1.036503
272.290713	140.792813	19.195546	-0.050646	1.026202
272.011642	133.339077	19.200551	-0.050589	1.015847
271.668554	125.889744	19.205555	-0.050521	1.005376
271.745189	118.387948	19.210560	-0.050530	0.994824
271.810768	110.871352	19.215565	-0.050537	0.984135
271.534113	103.446001	19.220570	-0.050481	0.973375
271.486769	96.006709	19.225575	-0.050467	0.962532
271.597278	88.557617	19.230579	-0.050483	0.951591
271.485487	81.155261	19.235584	-0.050458	0.940536
271.339428	73.783091	19.240589	-0.050426	0.929385
271.153617	66.428474	19.245594	-0.050386	0.918116
271.261405	59.262837	19.250599	-0.050402	0.907079