Fri Mar 12 12:04:05 2021


Number of Points = 3624

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.750866	0.128901	0.000000	0.000026	0.721126
0.667267	0.148094	0.005005	0.000042	0.721135
0.625157	0.151923	0.010010	0.000050	0.721127
0.759144	0.057068	0.015014	0.000025	0.720988
0.632292	0.027357	0.020019	0.000048	0.720885
0.653184	0.023141	0.025024	0.000044	0.720884
0.817875	-0.003944	0.030029	0.000014	0.720888
0.757076	0.002659	0.035034	0.000025	0.720880
0.601322	0.034263	0.040038	0.000054	0.720887
0.851211	-0.013904	0.045043	0.000008	0.720880
0.764328	0.001191	0.050048	0.000024	0.720879
0.561316	0.041925	0.055053	0.000062	0.720888
0.708257	0.011971	0.060058	0.000034	0.720881
0.751881	0.006564	0.065062	0.000026	0.720885
0.845886	-0.010672	0.070067	0.000009	0.720884
0.752702	0.004594	0.075072	0.000026	0.720882
0.582296	0.037459	0.080077	0.000058	0.720886
0.662772	-0.099195	0.085082	0.000043	0.720646
0.382043	-0.099694	0.090086	0.000095	0.720546
0.542996	-0.130397	0.095091	0.000065	0.720542
0.613738	-0.142023	0.100096	0.000052	0.720544
0.680482	-0.151430	0.105101	0.000040	0.720549
0.614608	-0.143921	0.110106	0.000052	0.720541
0.768407	-0.167562	0.115110	0.000024	0.720548
0.646303	-0.306564	0.120115	0.000046	0.720231
0.619255	-0.303233	0.125120	0.000051	0.720228
0.749247	-0.324063	0.130125	0.000027	0.720233
0.624246	-0.304477	0.135130	0.000051	0.720228
0.597996	-0.295937	0.140134	0.000055	0.720235
0.465462	-0.438834	0.145139	0.000080	0.719907
0.575112	-0.458222	0.150144	0.000060	0.719907
0.462205	-0.436906	0.155149	0.000081	0.719910
0.376674	-0.427000	0.160154	0.000097	0.719899
0.580424	-0.548021	0.165158	0.000059	0.719732
0.468523	-0.592417	0.170163	0.000080	0.719605
0.513845	-0.601061	0.175168	0.000071	0.719604
0.686919	-0.628340	0.180173	0.000039	0.719611
0.473411	-0.729560	0.185178	0.000079	0.719336
0.687613	-0.795195	0.190182	0.000039	0.719282
0.468724	-0.758604	0.195187	0.000080	0.719277
0.422946	-0.817426	0.200192	0.000089	0.719145
0.640358	-0.943008	0.205197	0.000048	0.718974
0.492787	-0.921610	0.210202	0.000076	0.718964
0.577432	-0.979623	0.215206	0.000060	0.718880
0.413127	-1.066529	0.220211	0.000091	0.718650
0.321929	-1.050859	0.225216	0.000108	0.718649
0.516580	-1.132320	0.230221	0.000072	0.718557
0.428777	-1.219005	0.235226	0.000088	0.718355
0.265423	-1.186688	0.240230	0.000118	0.718361
0.453005	-1.313385	0.245235	0.000084	0.718177
0.428611	-1.388712	0.250240	0.000088	0.718019
0.289729	-1.360992	0.255245	0.000114	0.718025
0.310040	-1.513300	0.260250	0.000110	0.717731
0.386181	-1.537188	0.265254	0.000096	0.717711
0.324869	-1.591556	0.270259	0.000108	0.717582
0.208691	-1.670402	0.275264	0.000129	0.717385
0.343671	-1.691503	0.280269	0.000104	0.717391
0.167456	-1.814158	0.285274	0.000137	0.717086
0.049500	-1.789300	0.290278	0.000159	0.717093
0.178339	-1.921463	0.295283	0.000135	0.716877
0.155767	-1.979421	0.300288	0.000140	0.716755
0.293530	-2.063051	0.305293	0.000114	0.716638
0.049334	-2.115767	0.310298	0.000160	0.716447
0.128611	-2.164359	0.315302	0.000145	0.716379
0.054647	-2.273528	0.320307	0.000159	0.716136
0.060353	-2.291348	0.325312	0.000158	0.716103
0.209459	-2.424333	0.330317	0.000130	0.715892
-0.534960	-2.303441	0.335322	0.000269	0.715869
-1.614711	-2.269608	0.340326	0.000470	0.715555
-2.396735	-2.132362	0.345331	0.000615	0.715551
-2.907534	-2.096653	0.350336	0.000710	0.715441
-3.195145	-2.147838	0.355341	0.000764	0.715238
-3.229976	-2.147476	0.360346	0.000770	0.715226
-3.595751	-2.107869	0.365350	0.000838	0.715175
-4.182422	-2.135904	0.370355	0.000948	0.714912
-4.064656	-2.158594	0.375360	0.000926	0.714909
-4.135720	-2.142924	0.380365	0.000939	0.714915
-4.471985	-2.198808	0.385370	0.001002	0.714685
-5.142963	-2.113534	0.390374	0.001127	0.714617
-5.351740	-2.078049	0.395379	0.001166	0.714614
-5.406439	-2.071192	0.400384	0.001176	0.714608
-5.321205	-2.214259	0.405389	0.001160	0.714354
-6.326824	-2.073786	0.410394	0.001347	0.714277
-6.305680	-2.073131	0.415398	0.001343	0.714286
-5.900296	-2.145137	0.420403	0.001268	0.714286
-6.268762	-2.158994	0.425408	0.001336	0.714128
-7.140041	-2.078733	0.430413	0.001499	0.713979
-7.085236	-2.091108	0.435418	0.001489	0.713974
-7.048465	-2.096814	0.440422	0.001482	0.713975
-7.123658	-2.082415	0.445427	0.001496	0.713977
-7.414707	-2.116074	0.450432	0.001550	0.713807
-8.129695	-2.060833	0.455437	0.001683	0.713664
-7.838746	-2.117439	0.460442	0.001629	0.713654
-8.192836	-2.052604	0.465446	0.001695	0.713658
-8.334332	-2.027530	0.470451	0.001721	0.713658
-8.110805	-2.070201	0.475456	0.001680	0.713652
-8.075483	-2.201723	0.480461	0.001673	0.713403
-9.297397	-2.004597	0.485466	0.001901	0.713362
-8.963155	-2.060675	0.490470	0.001838	0.713369
-8.379237	-2.166064	0.495475	0.001730	0.713366
-9.015250	-2.054648	0.500480	0.001848	0.713362
-8.611259	-2.178637	0.505485	0.001773	0.713259
-9.803351	-2.083198	0.510490	0.001995	0.713026
-9.812479	-2.079629	0.515494	0.001997	0.713030
-10.082907	-2.032053	0.520499	0.002047	0.713028
-9.925759	-2.061719	0.525504	0.002018	0.713025
-9.694789	-2.098576	0.530509	0.001975	0.713034
-10.330375	-1.990330	0.535514	0.002093	0.713024
-10.184216	-2.148621	0.540518	0.002066	0.712760
-10.596960	-2.097915	0.545523	0.002143	0.712715
-11.307311	-1.973481	0.550528	0.002275	0.712711
-10.772188	-2.064574	0.555533	0.002176	0.712719
-10.764644	-2.071269	0.560538	0.002174	0.712708
-10.715483	-2.076714	0.565542	0.002165	0.712715
-10.665403	-2.129327	0.570547	0.002156	0.712628
-11.877750	-2.034745	0.575552	0.002381	0.712386
-11.252507	-2.141899	0.580557	0.002265	0.712394
-11.891312	-2.033698	0.585562	0.002384	0.712383
-11.765501	-2.052176	0.590566	0.002361	0.712391
-11.261781	-2.141243	0.595571	0.002267	0.712392
-11.732950	-2.062754	0.600576	0.002355	0.712381
-11.654525	-2.165332	0.605581	0.002340	0.712205
-12.487966	-2.075209	0.610586	0.002495	0.712088
-12.278837	-2.109632	0.615590	0.002456	0.712094
-12.354588	-2.096858	0.620595	0.002470	0.712093
-12.440860	-2.085069	0.625600	0.002487	0.712085
-12.237725	-2.116348	0.630605	0.002449	0.712095
-12.637840	-2.073820	0.635610	0.002523	0.712038
-13.273447	-2.098961	0.640614	0.002642	0.711762
-12.737389	-2.193325	0.645619	0.002542	0.711764
-13.636660	-2.036704	0.650624	0.002709	0.711757
-13.379494	-2.077497	0.655629	0.002661	0.711767
-13.380064	-2.081955	0.660634	0.002662	0.711758
-13.376348	-2.080287	0.665638	0.002661	0.711762
-13.550369	-2.107467	0.670643	0.002693	0.711646
-14.646406	-2.010686	0.675648	0.002897	0.711450
-13.890227	-2.140560	0.680653	0.002757	0.711459
-14.511590	-2.034277	0.685658	0.002872	0.711451
-14.583690	-2.018356	0.690662	0.002886	0.711457
-14.083816	-2.108780	0.695667	0.002793	0.711454
-14.268803	-2.078613	0.700672	0.002827	0.711448
-14.141857	-2.135764	0.705677	0.002804	0.711379
-15.188835	-2.072599	0.710682	0.002999	0.711133
-14.960432	-2.110346	0.715686	0.002956	0.711139
-15.277067	-2.054528	0.720691	0.003015	0.711138
-15.440020	-2.026330	0.725696	0.003045	0.711136
-14.845278	-2.128145	0.730701	0.002935	0.711144
-15.413938	-2.030780	0.735706	0.003041	0.711136
-15.550452	-2.004946	0.740710	0.003066	0.711139
-15.433163	-2.159488	0.745715	0.003044	0.710873
-16.079154	-2.047205	0.750720	0.003165	0.710867
-16.299435	-2.002300	0.755725	0.003206	0.710878
-16.217063	-2.021260	0.760730	0.003190	0.710869
-15.958830	-2.065614	0.765734	0.003142	0.710873
-16.014587	-2.055658	0.770739	0.003153	0.710873
-16.214249	-2.022246	0.775744	0.003190	0.710868
-16.058088	-2.207229	0.780749	0.003161	0.710555
-16.832767	-2.081349	0.785754	0.003305	0.710530
-17.133913	-2.025045	0.790758	0.003361	0.710535
-16.768165	-2.090124	0.795763	0.003293	0.710536
-17.122481	-2.029893	0.800768	0.003359	0.710530
-17.211272	-2.009399	0.805773	0.003376	0.710539
-17.104302	-2.031294	0.810778	0.003356	0.710533
-17.655193	-2.087345	0.815782	0.003458	0.710225
-17.761914	-2.068658	0.820787	0.003478	0.710224
-18.249346	-1.985561	0.825792	0.003569	0.710217
-17.363729	-2.139225	0.830797	0.003404	0.710225
-17.694828	-2.084262	0.835802	0.003466	0.710217
-18.108519	-2.009268	0.840806	0.003543	0.710220
-17.807831	-2.061387	0.845811	0.003487	0.710222
-18.398992	-2.106286	0.850816	0.003597	0.709922
-18.923560	-2.024961	0.855821	0.003695	0.709898
-19.145121	-1.989359	0.860826	0.003736	0.709890
-18.621189	-2.080173	0.865830	0.003638	0.709895
-18.595411	-2.085332	0.870835	0.003634	0.709894
-19.020777	-2.013956	0.875840	0.003713	0.709885
-18.656874	-2.071916	0.880845	0.003645	0.709899
-18.775789	-2.138770	0.885850	0.003667	0.709723
-20.183293	-1.951797	0.890854	0.003929	0.709595
-19.471963	-2.077767	0.895859	0.003797	0.709596
-19.671129	-2.045608	0.900864	0.003834	0.709590
-19.729697	-2.030818	0.905869	0.003845	0.709598
-19.758111	-2.031041	0.910874	0.003850	0.709588
-19.478624	-2.078254	0.915878	0.003798	0.709593
-19.484986	-2.156894	0.920883	0.003799	0.709433
-20.721144	-2.022894	0.925888	0.004030	0.709261
-20.063067	-2.138947	0.930893	0.003907	0.709263
-20.373559	-2.085385	0.935898	0.003965	0.709259
-20.779668	-2.012675	0.940902	0.004041	0.709260
-20.411754	-2.076079	0.945907	0.003972	0.709264
-20.534061	-2.056250	0.950912	0.003995	0.709260
-20.880094	-2.092758	0.955917	0.004059	0.709064
-21.874987	-1.970399	0.960922	0.004245	0.708954
-21.486991	-2.039685	0.965926	0.004172	0.708953
-21.163599	-2.094767	0.970931	0.004112	0.708958
-21.823163	-1.981757	0.975936	0.004235	0.708949
-21.436210	-2.045983	0.980941	0.004163	0.708959
-21.404522	-2.053560	0.985946	0.004157	0.708955
-21.933587	-1.966264	0.990950	0.004256	0.708941
-22.358634	-2.039498	0.995955	0.004335	0.708642
-22.625759	-1.994947	1.000960	0.004385	0.708636
-22.548377	-2.005561	1.005965	0.004370	0.708643
-22.505093	-2.016840	1.010970	0.004362	0.708635
-22.537632	-2.009851	1.015974	0.004368	0.708638
-22.329991	-2.045007	1.020979	0.004330	0.708641
-22.555401	-2.008358	1.025984	0.004372	0.708634
-22.267271	-2.121528	1.030989	0.004318	0.708510
-23.218760	-2.032641	1.035994	0.004495	0.708349
-23.207701	-2.032410	1.040998	0.004493	0.708353
-23.437260	-1.990033	1.046003	0.004536	0.708356
-23.559634	-1.974550	1.051008	0.004559	0.708343
-23.126164	-2.044933	1.056013	0.004478	0.708357
-23.605169	-1.963822	1.061018	0.004567	0.708348
-23.485994	-2.037156	1.066022	0.004545	0.708244
-23.982768	-2.061712	1.071027	0.004638	0.708017
-24.307976	-2.006725	1.076032	0.004698	0.708011
-24.468504	-1.973382	1.081037	0.004728	0.708021
-24.123761	-2.038272	1.086042	0.004664	0.708014
-24.202714	-2.024491	1.091046	0.004679	0.708013
-24.380539	-1.991257	1.096051	0.004712	0.708016
-24.256703	-2.019927	1.101056	0.004689	0.708003
-24.363482	-2.148434	1.106061	0.004709	0.707707
-25.107407	-2.020018	1.111066	0.004847	0.707699
-25.166653	-2.008776	1.116070	0.004858	0.707700
-24.632143	-2.100758	1.121075	0.004759	0.707706
-25.255186	-1.994511	1.126080	0.004875	0.707697
-25.050427	-2.024839	1.131085	0.004837	0.707709
-25.048710	-2.072441	1.136090	0.004836	0.707614
-26.116340	-1.998520	1.141094	0.005035	0.707381
-25.770460	-2.058206	1.146099	0.004971	0.707385
-25.950845	-2.029962	1.151104	0.005004	0.707377
-25.772102	-2.058145	1.156109	0.004971	0.707384
-26.140487	-1.996040	1.161114	0.005040	0.707377
-26.068449	-2.006604	1.166118	0.005026	0.707381
-25.413517	-2.168050	1.171123	0.004904	0.707292
-26.885750	-2.013086	1.176128	0.005179	0.707076
-26.733629	-2.034388	1.181133	0.005150	0.707088
-26.729436	-2.037370	1.186138	0.005149	0.707083
-26.476229	-2.082988	1.191142	0.005102	0.707082
-26.544250	-2.068394	1.196147	0.005115	0.707087
-27.033621	-1.984254	1.201152	0.005206	0.707081
-26.750247	-2.129635	1.206157	0.005153	0.706890
-27.822738	-2.006803	1.211162	0.005353	0.706753
-27.798324	-2.010279	1.216166	0.005349	0.706755
-27.223993	-2.110653	1.221171	0.005242	0.706759
-27.707346	-2.028748	1.226176	0.005332	0.706750
-27.676728	-2.031892	1.231181	0.005326	0.706755
-27.473038	-2.067325	1.236186	0.005288	0.706756
-27.802347	-2.119648	1.241190	0.005350	0.706533
-28.534721	-2.029671	1.246195	0.005486	0.706452
-28.555583	-2.029117	1.251200	0.005490	0.706445
-28.415101	-2.051186	1.256205	0.005464	0.706451
-28.645519	-2.013394	1.261210	0.005507	0.706445
-28.849380	-1.977888	1.266214	0.005545	0.706443
-28.008226	-2.126643	1.271219	0.005388	0.706445
-28.700737	-2.126946	1.276224	0.005517	0.706196
-29.789148	-1.964316	1.281229	0.005720	0.706133
-29.590329	-2.002455	1.286234	0.005683	0.706128
-29.160991	-2.080598	1.291238	0.005603	0.706125
-29.324551	-2.048549	1.296243	0.005633	0.706130
-29.642498	-1.995617	1.301248	0.005692	0.706123
-29.275168	-2.055913	1.306253	0.005624	0.706133
-29.562908	-2.086315	1.311258	0.005678	0.705969
-30.548757	-1.962833	1.316262	0.005861	0.705864
-30.050612	-2.049557	1.321267	0.005768	0.705868
-30.220023	-2.025119	1.326272	0.005800	0.705856
-30.430873	-1.982816	1.331277	0.005839	0.705866
-30.179729	-2.031368	1.336282	0.005793	0.705858
-30.186774	-2.028772	1.341286	0.005794	0.705861
-30.317283	-2.116811	1.346291	0.005818	0.705637
-31.419995	-1.977897	1.351296	0.006024	0.705521
-30.904867	-2.065440	1.356301	0.005928	0.705529
-30.943019	-2.062032	1.361306	0.005935	0.705522
-31.545538	-1.954214	1.366310	0.006047	0.705523
-30.937645	-2.060505	1.371315	0.005934	0.705527
-31.122209	-2.032237	1.376320	0.005968	0.705518
-31.610624	-2.053622	1.381325	0.006059	0.705300
-32.442674	-1.949279	1.386330	0.006214	0.705211
-32.338058	-1.971049	1.391334	0.006195	0.705205
-31.902361	-2.044436	1.396339	0.006114	0.705213
-32.589030	-1.926228	1.401344	0.006241	0.705205
-32.310143	-1.970575	1.406349	0.006189	0.705216
-31.925352	-2.042253	1.411354	0.006118	0.705209
-32.346265	-1.974329	1.416358	0.006196	0.705195
-32.765203	-2.050560	1.421363	0.006274	0.704891
-32.921359	-2.028514	1.426368	0.006303	0.704879
-33.097056	-1.992404	1.431373	0.006336	0.704889
-32.924311	-2.025466	1.436378	0.006304	0.704884
-32.951887	-2.020878	1.441382	0.006309	0.704884
-32.884467	-2.027723	1.446387	0.006297	0.704894
-33.468619	-1.927747	1.451392	0.006405	0.704886
-33.298949	-2.081959	1.456397	0.006374	0.704636
-33.609979	-2.050777	1.461402	0.006432	0.704587
-34.177274	-1.948457	1.466406	0.006537	0.704589
-33.661412	-2.039164	1.471411	0.006441	0.704592
-33.719989	-2.032032	1.476416	0.006452	0.704585
-33.939889	-1.990135	1.481421	0.006493	0.704590
-33.858764	-2.010155	1.486426	0.006478	0.704579
-34.732345	-2.015179	1.491430	0.006641	0.704255
-34.508374	-2.052766	1.496435	0.006599	0.704260
-35.143631	-1.941115	1.501440	0.006717	0.704257
-34.813397	-1.996214	1.506445	0.006656	0.704264
-34.631984	-2.030473	1.511450	0.006622	0.704260
-34.975454	-1.970107	1.516454	0.006686	0.704258
-34.417171	-2.066135	1.521459	0.006582	0.704265
-35.081937	-2.086600	1.526464	0.006706	0.703985
-35.907083	-1.953321	1.531469	0.006860	0.703957
-35.797685	-1.974701	1.536474	0.006839	0.703953
-35.556455	-2.017921	1.541478	0.006795	0.703953
-35.445972	-2.035973	1.546483	0.006774	0.703956
-35.798039	-1.978369	1.551488	0.006840	0.703946
-35.696944	-1.992773	1.556493	0.006821	0.703953
-35.864608	-2.076383	1.561498	0.006852	0.703724
-36.935833	-1.931483	1.566502	0.007051	0.703631
-36.484994	-2.007472	1.571507	0.006968	0.703640
-36.114482	-2.076953	1.576512	0.006899	0.703633
-36.419317	-2.021190	1.581517	0.006955	0.703636
-36.510762	-2.006104	1.586522	0.006972	0.703633
-36.333508	-2.037376	1.591526	0.006939	0.703634
-36.663978	-2.112359	1.596531	0.007001	0.703363
-37.246419	-2.021445	1.601536	0.007110	0.703337
-37.383112	-1.992259	1.606541	0.007135	0.703347
-36.991995	-2.064563	1.611546	0.007062	0.703342
-37.483068	-1.977759	1.616550	0.007154	0.703340
-37.211165	-2.024207	1.621555	0.007103	0.703344
-37.314703	-2.058923	1.626560	0.007122	0.703237
-38.354796	-1.987554	1.631565	0.007316	0.703006
-38.223130	-2.012439	1.636570	0.007292	0.703004
-38.449841	-1.971958	1.641574	0.007334	0.703004
-38.069466	-2.035507	1.646579	0.007263	0.703012
-38.307972	-1.997907	1.651584	0.007307	0.703002
-38.162962	-2.019723	1.656589	0.007280	0.703010
-38.058603	-2.071426	1.661594	0.007261	0.702943
-39.277451	-1.979333	1.666598	0.007488	0.702690
-38.858706	-2.050422	1.671603	0.007410	0.702698
-39.273073	-1.980420	1.676608	0.007487	0.702690
-38.997509	-2.026829	1.681613	0.007436	0.702695
-38.987804	-2.030123	1.686618	0.007434	0.702692
-39.243680	-1.985676	1.691622	0.007482	0.702690
-38.688276	-2.131150	1.696627	0.007378	0.702596
-40.243310	-1.968117	1.701632	0.007668	0.702365
-39.860970	-2.033028	1.706637	0.007597	0.702371
-39.734745	-2.056556	1.711642	0.007573	0.702369
-40.028527	-2.005388	1.716646	0.007628	0.702367
-39.923223	-2.020978	1.721651	0.007608	0.702373
-40.110763	-1.992073	1.726656	0.007643	0.702364
-39.933274	-2.066011	1.731661	0.007610	0.702278
-40.939240	-1.988319	1.736666	0.007798	0.702073
-40.773656	-2.020178	1.741670	0.007767	0.702068
-40.638981	-2.039193	1.746675	0.007742	0.702078
-40.865389	-2.003548	1.751680	0.007784	0.702068
-40.697610	-2.031013	1.756685	0.007753	0.702073
-40.715359	-2.027172	1.761690	0.007756	0.702075
-40.947225	-2.057269	1.766694	0.007799	0.701930
-41.769641	-2.000524	1.771699	0.007952	0.701748
-41.450679	-2.063203	1.776704	0.007893	0.701736
-41.462072	-2.055404	1.781709	0.007895	0.701748
-41.884772	-1.980202	1.786714	0.007974	0.701748
-41.911040	-1.977696	1.791718	0.007979	0.701743
-41.472559	-2.052199	1.796723	0.007897	0.701751
-42.030032	-2.019418	1.801728	0.008001	0.701616
-42.868975	-1.957406	1.806733	0.008157	0.701438
-42.101029	-2.094786	1.811738	0.008014	0.701437
-42.465481	-2.032708	1.816742	0.008082	0.701431
-42.534962	-2.016596	1.821747	0.008095	0.701439
-42.587336	-2.011516	1.826752	0.008105	0.701430
-42.277852	-2.062595	1.831757	0.008047	0.701439
-42.583558	-2.112643	1.836762	0.008104	0.701227
-43.672346	-1.970572	1.841766	0.008307	0.701121
-43.474136	-2.002775	1.846771	0.008270	0.701128
-43.395198	-2.020954	1.851776	0.008255	0.701119
-43.604007	-1.980153	1.856781	0.008294	0.701126
-43.286494	-2.037562	1.861786	0.008235	0.701125
-43.445032	-2.012353	1.866790	0.008265	0.701119
-43.602246	-2.054579	1.871795	0.008294	0.700976
-44.236881	-1.993665	1.876800	0.008412	0.700870
-43.983491	-2.037020	1.881805	0.008365	0.700874
-44.169874	-2.005573	1.886810	0.008400	0.700870
-44.616465	-1.925452	1.891814	0.008483	0.700871
-43.787920	-2.067288	1.896819	0.008329	0.700883
-43.951617	-2.050056	1.901824	0.008359	0.700859
-44.985286	-2.024294	1.906829	0.008552	0.700538
-44.945123	-2.030974	1.911834	0.008544	0.700538
-45.122776	-2.001044	1.916838	0.008577	0.700535
-44.796834	-2.054643	1.921843	0.008517	0.700544
-45.235696	-1.981866	1.926848	0.008598	0.700533
-44.877177	-2.044779	1.931853	0.008532	0.700535
-44.529784	-2.171734	1.936858	0.008467	0.700403
-46.172748	-1.971902	1.941862	0.008773	0.700214
-45.761813	-2.042048	1.946867	0.008697	0.700220
-46.048615	-1.993228	1.951872	0.008750	0.700216
-46.084718	-1.984153	1.956877	0.008757	0.700221
-45.868880	-2.023123	1.961882	0.008717	0.700220
-45.788582	-2.040386	1.966886	0.008702	0.700214
-45.944631	-2.108924	1.971891	0.008731	0.700018
-46.886759	-2.003669	1.976896	0.008906	0.699891
-46.580971	-2.057220	1.981901	0.008849	0.699893
-46.598559	-2.055255	1.986906	0.008853	0.699891
-47.196303	-1.950289	1.991910	0.008964	0.699887
-46.333895	-2.098144	1.996915	0.008803	0.699899
-46.793398	-2.080419	2.001920	0.008889	0.699769
-47.798306	-1.986791	2.011917	0.009076	0.699595
-47.602707	-2.020363	2.021914	0.009040	0.699598
-47.367549	-2.061798	2.031910	0.008996	0.699599
-47.703130	-2.002487	2.041907	0.009058	0.699597
-47.605018	-2.022253	2.051904	0.009040	0.699593
-47.425955	-2.054800	2.061901	0.009007	0.699591
-47.484617	-2.042757	2.071898	0.009018	0.699594
-47.284396	-2.077962	2.081894	0.008981	0.699595
-47.698830	-2.003587	2.091891	0.009058	0.699596
-47.430670	-2.051100	2.101888	0.009008	0.699597
-47.715872	-1.993882	2.111885	0.009061	0.699610
-46.595269	-2.054218	2.121882	0.008853	0.699893
-46.387390	-2.092597	2.131878	0.008814	0.699890
-46.615989	-2.050556	2.141875	0.008856	0.699892
-46.731351	-2.029287	2.151872	0.008878	0.699894
-46.774969	-2.021005	2.161869	0.008886	0.699895
-46.743460	-2.014373	2.171866	0.008880	0.699920
-45.841527	-2.025895	2.181862	0.008712	0.700222
-45.801957	-2.034683	2.191859	0.008705	0.700219
-45.704026	-2.053186	2.201856	0.008687	0.700217
-46.140467	-1.975505	2.211853	0.008768	0.700216
-45.131308	-2.029210	2.221850	0.008580	0.700472
-45.023616	-2.018459	2.231846	0.008560	0.700533
-44.999379	-2.021467	2.241843	0.008556	0.700535
-45.030473	-2.018387	2.251840	0.008562	0.700530
-44.492860	-1.962831	2.261837	0.008462	0.700837
-44.089505	-2.016977	2.271834	0.008387	0.700873
-43.741508	-2.079763	2.281830	0.008322	0.700871
-44.190574	-1.990347	2.291827	0.008405	0.700890
-43.566858	-1.988340	2.301824	0.008289	0.701120
-43.454855	-2.008233	2.311821	0.008269	0.701120
-43.327003	-2.031608	2.321818	0.008245	0.701118
-42.921228	-1.988266	2.331814	0.008169	0.701353
-42.618753	-2.001361	2.341811	0.008113	0.701435
-42.543418	-2.016915	2.351808	0.008099	0.701431
-42.674382	-1.935611	2.361805	0.008123	0.701548
-41.591907	-2.031823	2.371802	0.007922	0.701744
-41.540120	-2.040398	2.381798	0.007912	0.701745
-41.648262	-2.022657	2.391795	0.007933	0.701742
-40.878944	-2.010917	2.401792	0.007789	0.702043
-40.943846	-1.985624	2.411789	0.007801	0.702071
-40.517386	-2.061664	2.421786	0.007722	0.702071
-40.797189	-1.945844	2.431782	0.007774	0.702204
-39.899580	-2.024182	2.441779	0.007607	0.702369
-39.848898	-2.033641	2.451776	0.007598	0.702368
-40.221684	-1.958780	2.461773	0.007667	0.702385
-39.075297	-2.011185	2.471770	0.007454	0.702692
-39.093559	-2.007617	2.481766	0.007457	0.702693
-38.985300	-2.027807	2.491763	0.007437	0.702691
-38.762862	-1.980783	2.501760	0.007396	0.702866
-38.274202	-2.000124	2.511757	0.007305	0.703003
-38.100223	-2.029401	2.521754	0.007272	0.703006
-38.277783	-1.980366	2.531750	0.007306	0.703041
-37.462367	-1.975615	2.541747	0.007154	0.703344
-37.271597	-2.010400	2.551744	0.007118	0.703343
-37.259993	-2.012699	2.561741	0.007116	0.703342
-36.721575	-2.031490	2.571738	0.007016	0.703498
-36.472174	-2.009113	2.581734	0.006970	0.703633
-36.456929	-2.011713	2.591731	0.006967	0.703633
-36.676762	-1.952337	2.601728	0.007008	0.703673
-35.759000	-1.979985	2.611725	0.006837	0.703948
-35.568492	-2.013095	2.621722	0.006801	0.703949
-35.566771	-2.013283	2.631718	0.006801	0.703949
-34.836261	-2.032876	2.641715	0.006665	0.704173
-34.766119	-2.003863	2.651712	0.006652	0.704256
-34.514600	-2.048703	2.661709	0.006605	0.704256
-34.478619	-2.056123	2.671706	0.006599	0.704254
-34.105510	-1.960017	2.681702	0.006529	0.704582
-33.755747	-2.020547	2.691699	0.006464	0.704585
-33.965476	-1.982883	2.701696	0.006503	0.704586
-33.209579	-2.023613	2.711693	0.006363	0.704775
-33.070096	-1.993616	2.721690	0.006337	0.704885
-32.895030	-2.024435	2.731686	0.006304	0.704886
-32.827782	-2.026604	2.741683	0.006292	0.704906
-32.268323	-1.976098	2.751680	0.006188	0.705208
-32.025584	-2.019292	2.761677	0.006142	0.705208
-31.950493	-2.030851	2.771674	0.006128	0.705212
-31.705961	-1.983201	2.781670	0.006083	0.705396
-30.942191	-2.054500	2.791667	0.005941	0.705526
-31.447167	-1.966379	2.801664	0.006035	0.705522
-30.930683	-2.053517	2.811661	0.005939	0.705532
-30.357967	-1.989686	2.821658	0.005832	0.705866
-30.100876	-2.035980	2.831654	0.005784	0.705865
-30.227354	-2.014636	2.841651	0.005808	0.705862
-30.145677	-1.977936	2.851648	0.005793	0.705965
-29.467186	-2.017802	2.861645	0.005666	0.706128
-29.431304	-2.023768	2.871642	0.005660	0.706129
-29.505157	-1.997967	2.881638	0.005674	0.706154
-28.750381	-1.986385	2.891635	0.005533	0.706448
-28.674405	-2.001443	2.901632	0.005519	0.706445
-28.541024	-2.026772	2.911629	0.005494	0.706441
-28.284841	-1.959437	2.921626	0.005447	0.706668
-27.757880	-2.012048	2.931622	0.005348	0.706751
-27.919271	-1.982771	2.941619	0.005379	0.706752
-27.473514	-1.999887	2.951616	0.005296	0.706877
-26.789304	-2.021230	2.961613	0.005168	0.707079
-26.821856	-2.014608	2.971610	0.005174	0.707081
-26.751828	-2.026777	2.981606	0.005161	0.707081
-26.195162	-2.001988	2.991603	0.005058	0.707330
-26.057600	-2.003879	3.001600	0.005032	0.707376
-26.075645	-2.001361	3.011597	0.005036	0.707374
-25.864224	-1.974232	3.021594	0.004996	0.707504
-24.915410	-2.045173	3.031590	0.004820	0.707701
-25.178750	-1.997687	3.041587	0.004869	0.707702
-25.067863	-2.019904	3.051584	0.004848	0.707697
-24.522601	-1.980960	3.061581	0.004747	0.707970
-24.315223	-1.995116	3.071578	0.004708	0.708015
-24.231874	-2.009853	3.081574	0.004693	0.708016
-24.161941	-1.936193	3.091571	0.004680	0.708188
-23.431904	-1.985467	3.101568	0.004544	0.708350
-23.371777	-1.995402	3.111565	0.004533	0.708352
-23.287994	-2.009474	3.121562	0.004517	0.708353
-22.408394	-2.021945	3.131558	0.004353	0.708642
-22.657709	-1.976298	3.141555	0.004400	0.708645
-22.487303	-2.007877	3.151552	0.004368	0.708642
-22.274307	-1.967946	3.161549	0.004328	0.708798
-21.550851	-2.015579	3.171546	0.004194	0.708961
-21.752322	-1.980372	3.181542	0.004231	0.708959
-21.708886	-1.980734	3.191539	0.004223	0.708974
-20.882446	-1.983396	3.201536	0.004069	0.709263
-21.040062	-1.955303	3.211533	0.004099	0.709263
-20.686515	-2.017608	3.221530	0.004033	0.709265
-20.153255	-2.003742	3.231526	0.003934	0.709482
-20.207902	-1.936880	3.241523	0.003944	0.709597
-19.999602	-1.974860	3.251520	0.003905	0.709595
-19.951289	-1.944392	3.261517	0.003896	0.709673
-19.139601	-1.979102	3.271514	0.003745	0.709893
-18.991526	-2.004863	3.281510	0.003718	0.709894
-19.047494	-1.995160	3.291507	0.003728	0.709893
-18.209510	-2.016451	3.301504	0.003572	0.710149
-18.355570	-1.957647	3.311501	0.003599	0.710214
-18.218538	-1.982457	3.321498	0.003574	0.710214
-18.218909	-1.921920	3.331494	0.003574	0.710334
-17.448298	-1.959956	3.341491	0.003431	0.710533
-17.309459	-1.985870	3.351488	0.003405	0.710530
-17.102794	-2.021953	3.361485	0.003366	0.710532
-16.576061	-1.987924	3.371482	0.003268	0.710787
-16.358899	-1.985205	3.381478	0.003228	0.710869
-16.268717	-2.001548	3.391475	0.003211	0.710869
-16.019965	-2.044817	3.401472	0.003165	0.710871
-15.769984	-1.957410	3.411469	0.003118	0.711134
-15.233204	-2.052238	3.421466	0.003018	0.711136
-15.189857	-2.058394	3.431462	0.003010	0.711139
-15.240807	-2.005800	3.441459	0.003020	0.711225
-14.537764	-2.017159	3.451456	0.002889	0.711453
-14.450605	-2.032414	3.461453	0.002873	0.711453
-14.332922	-2.052677	3.471450	0.002851	0.711454
-13.947094	-2.018639	3.481446	0.002779	0.711659
-13.474938	-2.052561	3.491443	0.002691	0.711759
-13.673715	-2.015532	3.501440	0.002728	0.711763
-13.744696	-1.986928	3.511437	0.002742	0.711794
-12.672511	-2.028825	3.521434	0.002542	0.712091
-12.632946	-2.034657	3.531430	0.002535	0.712094
-12.446683	-2.069531	3.541427	0.002500	0.712090
-12.576834	-1.983858	3.551424	0.002524	0.712215
-11.721273	-2.049684	3.561421	0.002365	0.712387
-11.617189	-2.068502	3.571418	0.002346	0.712387
-11.816052	-2.032753	3.581414	0.002383	0.712387
-10.939563	-2.059856	3.591411	0.002220	0.712644
-10.954048	-2.024773	3.601408	0.002222	0.712709
-10.741119	-2.061886	3.611405	0.002183	0.712710
-10.533116	-2.097572	3.621402	0.002144	0.712713
-10.020756	-2.030434	3.631398	0.002049	0.713028
-9.680746	-2.092309	3.641395	0.001986	0.713026
-9.989071	-2.040003	3.651392	0.002043	0.713020
-9.845447	-2.014534	3.661389	0.002016	0.713122
-8.743793	-2.093357	3.671386	0.001811	0.713355
-8.913541	-2.060085	3.681382	0.001843	0.713361
-8.941613	-2.055278	3.691379	0.001848	0.713361
-8.585362	-2.019014	3.701376	0.001782	0.713559
-8.086700	-2.063757	3.711373	0.001689	0.713647
-8.053113	-2.068206	3.721370	0.001683	0.713650
-8.035857	-2.048479	3.731366	0.001680	0.713695
-7.175392	-2.064481	3.741363	0.001520	0.713968
-7.258727	-2.050576	3.751360	0.001535	0.713966
-7.102478	-2.076052	3.761357	0.001506	0.713970
-6.806898	-2.046391	3.771354	0.001451	0.714134
-6.073280	-2.103761	3.781350	0.001315	0.714280
-6.252434	-2.072077	3.791347	0.001348	0.714279
-6.313268	-2.062063	3.801344	0.001359	0.714277
-5.413191	-2.083700	3.811341	0.001192	0.714553
-5.050524	-2.120205	3.821338	0.001124	0.714608
-5.204215	-2.090854	3.831334	0.001153	0.714612
-5.138301	-2.103540	3.841331	0.001141	0.714610
-4.788658	-2.029564	3.851328	0.001076	0.714881
-4.308835	-2.102008	3.861325	0.000986	0.714906
-4.438271	-2.077175	3.871322	0.001010	0.714910
-4.188970	-2.060856	3.881318	0.000964	0.715030
-3.345312	-2.108923	3.891315	0.000807	0.715233
-3.427024	-2.095507	3.901312	0.000822	0.715231
-3.367258	-2.105798	3.911309	0.000811	0.715231
-3.045773	-2.051707	3.921306	0.000751	0.715452
-2.718782	-2.061713	3.931302	0.000691	0.715548
-2.701364	-2.065090	3.941299	0.000687	0.715547
-2.509882	-2.051303	3.951296	0.000652	0.715642
-1.750137	-2.063700	3.961293	0.000510	0.715885
-1.817344	-2.051805	3.971290	0.000523	0.715885
-1.639731	-2.084192	3.981286	0.000490	0.715884
-1.673919	-1.980914	3.991283	0.000496	0.716076
-1.429549	-1.994659	4.001280	0.000451	0.716135
-1.186398	-2.038799	4.011277	0.000406	0.716133
-1.162412	-1.915344	4.021274	0.000401	0.716386
-1.189345	-1.877116	4.031270	0.000406	0.716452
-1.154231	-1.842832	4.041267	0.000400	0.716533
-1.113736	-1.736777	4.051264	0.000392	0.716757
-1.144987	-1.709926	4.061261	0.000398	0.716799
-1.040289	-1.583189	4.071258	0.000378	0.717086
-1.151989	-1.525167	4.081254	0.000399	0.717162
-0.931854	-1.453065	4.091251	0.000358	0.717382
-0.872505	-1.384625	4.101248	0.000347	0.717538
-0.812032	-1.311978	4.111245	0.000336	0.717703
-0.727044	-1.190366	4.121242	0.000320	0.717973
-0.676296	-1.123611	4.131238	0.000310	0.718123
-0.668511	-1.008232	4.141235	0.000309	0.718353
-0.592831	-0.894060	4.151232	0.000295	0.718605
-0.744431	-0.769382	4.161229	0.000323	0.718798
-0.420078	-0.715700	4.171226	0.000263	0.719018
-0.499432	-0.572094	4.181222	0.000277	0.719273
-0.449146	-0.426240	4.191219	0.000268	0.719578
-0.301227	-0.330465	4.201216	0.000240	0.719819
-0.111936	-0.237295	4.211213	0.000205	0.720069
-0.162385	-0.088012	4.221210	0.000214	0.720345
-0.223880	0.074447	4.231206	0.000226	0.720643
0.000000	0.202190	4.241203	0.000184	0.720973
0.047197	0.805724	4.246208	0.000175	0.722176
0.161561	2.056536	4.251213	0.000153	0.724668
0.397672	3.877061	4.256218	0.000108	0.728305
0.549503	6.263697	4.261222	0.000078	0.732991
0.643627	9.165454	4.266227	0.000059	0.738618
0.970448	12.505192	4.271232	-0.000004	0.745115
1.391664	16.283870	4.276237	-0.000085	0.752415
1.764477	20.477446	4.281242	-0.000157	0.760404
2.214416	25.053345	4.286246	-0.000244	0.769040
2.425393	30.045018	4.291251	-0.000287	0.778260
2.991725	35.316924	4.296256	-0.000396	0.787991
3.443945	40.922394	4.301261	-0.000483	0.798160
3.788645	46.857143	4.306266	-0.000551	0.808745
4.048723	53.084860	4.311270	-0.000604	0.819674
4.374166	59.568095	4.316275	-0.000669	0.830916
4.910233	66.242501	4.321280	-0.000773	0.842391
5.086567	73.192998	4.326285	-0.000810	0.854066
5.435231	80.319075	4.331290	-0.000880	0.865920
5.847399	87.618831	4.336294	-0.000961	0.877912
6.356869	95.075866	4.341299	-0.001061	0.890021
7.146281	102.647243	4.346304	-0.001213	0.902224
9.170943	110.168815	4.351309	-0.001595	0.914522
9.709957	118.079266	4.356314	-0.001700	0.926853
10.050526	126.141696	4.361318	-0.001769	0.939198
10.758243	134.239811	4.366323	-0.001906	0.951532
11.391487	142.442525	4.371328	-0.002029	0.963843
15.143528	150.203989	4.376333	-0.002733	0.976147
18.837164	158.162508	4.381338	-0.003426	0.988563
19.559871	166.686604	4.386342	-0.003566	1.000893
19.944415	175.287867	4.391347	-0.003643	1.013097
20.797334	183.838400	4.396352	-0.003807	1.025199
21.434104	192.452349	4.401357	-0.003931	1.037194
22.566042	201.000952	4.406362	-0.004148	1.049079
24.048530	209.530712	4.411366	-0.004429	1.060886
24.863081	218.205665	4.416371	-0.004587	1.072602
25.326719	226.939540	4.421376	-0.004679	1.084189
26.318993	235.580843	4.426381	-0.004869	1.095651
27.877748	244.129272	4.431386	-0.005165	1.107000
28.763083	252.814778	4.436390	-0.005335	1.118259
29.515254	261.501466	4.441395	-0.005481	1.129379
30.327642	270.192111	4.446400	-0.005638	1.140408
30.680735	278.953421	4.451405	-0.005709	1.151320
31.432714	287.623952	4.456410	-0.005855	1.162103
32.016191	296.291699	4.461414	-0.005969	1.172748
32.469327	304.957236	4.466419	-0.006059	1.183267
33.774934	313.489014	4.471424	-0.006308	1.193707
34.484722	322.085009	4.476429	-0.006446	1.204013
35.210076	330.687531	4.481434	-0.006586	1.214241
35.959862	339.269008	4.486438	-0.006732	1.224364
36.760184	347.850371	4.491443	-0.006886	1.234413
37.654859	356.370307	4.496448	-0.007058	1.244329
38.353923	364.917386	4.501453	-0.007194	1.254159
39.076877	373.445111	4.506458	-0.007334	1.263895
39.910797	381.950263	4.511462	-0.007495	1.273552
40.430271	390.478882	4.516467	-0.007597	1.283104
40.699277	399.049402	4.521472	-0.007653	1.292584
41.585137	407.468775	4.526477	-0.007823	1.301944
42.912353	415.914606	4.531482	-0.008076	1.311345
43.825197	424.386644	4.536486	-0.008251	1.320632
44.012704	432.886779	4.541491	-0.008292	1.329754
44.972976	441.279311	4.546496	-0.008476	1.338837
45.860498	449.651751	4.551501	-0.008647	1.347825
46.406729	458.094724	4.556506	-0.008754	1.356767
46.943878	466.484688	4.561510	-0.008859	1.365593
47.489528	474.890446	4.566515	-0.008966	1.374380
48.123703	483.269171	4.571520	-0.009090	1.383099
48.525890	491.673478	4.576525	-0.009170	1.391749
49.644848	499.953132	4.581530	-0.009384	1.400340
50.084760	508.334324	4.586534	-0.009471	1.408867
50.556721	516.700667	4.591539	-0.009565	1.417333
51.255384	525.023953	4.596544	-0.009700	1.425743
51.699004	533.379655	4.601549	-0.009788	1.434094
52.481825	541.669271	4.606554	-0.009939	1.442386
53.007183	549.995947	4.611558	-0.010043	1.450626
53.772656	558.272942	4.616563	-0.010190	1.458809
54.724745	566.532613	4.621568	-0.010373	1.466958
55.235900	574.905542	4.626573	-0.010474	1.475102
55.937441	583.168798	4.631578	-0.010610	1.483126
56.347046	591.478560	4.636582	-0.010691	1.491105
56.669985	599.800029	4.641587	-0.010757	1.499039
57.416717	608.045938	4.646592	-0.010901	1.506925
58.294556	616.278641	4.651597	-0.011070	1.514777
58.452890	624.602225	4.656602	-0.011105	1.522565
59.057608	632.851599	4.661606	-0.011223	1.530311
59.563900	641.112957	4.666611	-0.011323	1.538014
60.099096	649.360290	4.671616	-0.011428	1.545670
60.502175	657.648207	4.676621	-0.011508	1.553305
61.050625	665.871710	4.681626	-0.011615	1.560866
61.748334	674.068648	4.686630	-0.011751	1.568388
62.271104	682.314431	4.691635	-0.011853	1.575892
63.021928	690.510213	4.696640	-0.011998	1.583349
63.366920	698.777233	4.701645	-0.012068	1.590776
63.623282	707.051271	4.706650	-0.012121	1.598162
64.025642	715.259269	4.711654	-0.012201	1.605476
64.514000	723.477911	4.716659	-0.012298	1.612778
64.899430	731.711077	4.721664	-0.012375	1.620045
65.509064	739.888257	4.726669	-0.012494	1.627263
65.982693	748.160059	4.731674	-0.012587	1.634511
66.421176	756.340495	4.736678	-0.012674	1.641643
67.161669	764.478737	4.741683	-0.012817	1.648750
67.832341	772.666804	4.746688	-0.012947	1.655859
68.136486	780.867532	4.751693	-0.013009	1.662899
68.726941	789.056456	4.756698	-0.013125	1.669937
69.402035	797.229290	4.761702	-0.013256	1.676943
70.432575	805.332512	4.766707	-0.013453	1.683909
70.767420	813.577484	4.771712	-0.013521	1.690872
70.856351	821.819701	4.776717	-0.013542	1.697772
71.557157	829.972360	4.781722	-0.013678	1.704649
72.082682	838.168223	4.786726	-0.013781	1.711512
72.395916	846.359938	4.791731	-0.013845	1.718316
72.847676	854.523152	4.796736	-0.013934	1.725088
73.218046	862.698880	4.801741	-0.014009	1.731832
73.485678	870.905178	4.806746	-0.014064	1.738563
73.984796	879.040761	4.811750	-0.014162	1.745239
74.207770	887.236347	4.816755	-0.014209	1.751903
74.704807	895.386666	4.821760	-0.014307	1.758540
74.871436	903.557762	4.826765	-0.014343	1.765127
75.293331	911.718837	4.831770	-0.014427	1.771713
76.079362	919.829369	4.836774	-0.014579	1.778280
76.556080	927.961481	4.841779	-0.014673	1.784801
76.949856	936.182924	4.846784	-0.014751	1.791359
77.638680	944.306117	4.851789	-0.014885	1.797852
78.149152	952.420329	4.856794	-0.014985	1.804292
78.600052	960.574858	4.861798	-0.015074	1.810733
78.876826	968.728664	4.866803	-0.015131	1.817130
79.572592	976.835425	4.871808	-0.015266	1.823518
80.011111	984.975603	4.876813	-0.015353	1.829878
80.514751	993.117927	4.881818	-0.015452	1.836226
81.265325	1001.224378	4.886822	-0.015597	1.842553
81.520630	1009.400536	4.891827	-0.015650	1.848854
81.848883	1017.573422	4.896832	-0.015716	1.855139
82.195030	1025.706958	4.901837	-0.015786	1.861375
82.648403	1033.841638	4.906842	-0.015876	1.867604
83.013633	1042.026459	4.911846	-0.015949	1.873839
83.566526	1050.108914	4.916851	-0.016057	1.879998
84.164048	1058.215555	4.921856	-0.016174	1.886160
84.417815	1066.376694	4.926861	-0.016226	1.892303
84.859921	1074.498746	4.931866	-0.016314	1.898419
85.543425	1082.579507	4.936870	-0.016446	1.904511
85.969586	1090.711836	4.941875	-0.016531	1.910593
86.337482	1098.864493	4.946880	-0.016605	1.916664
86.634256	1106.978174	4.951885	-0.016665	1.922679
87.065442	1115.108122	4.956890	-0.016751	1.928702
87.471829	1123.246281	4.961894	-0.016832	1.934710
87.865763	1131.353122	4.966899	-0.016911	1.940674
88.528554	1139.453675	4.971904	-0.017039	1.946645
88.806860	1147.628555	4.976909	-0.017096	1.952610
89.293831	1155.731537	4.981914	-0.017192	1.958527
89.830703	1163.808658	4.986918	-0.017297	1.964413
90.162385	1171.918762	4.991923	-0.017364	1.970282
90.600675	1180.057058	4.996928	-0.017451	1.976166
90.828879	1188.161900	5.001933	-0.017499	1.981986
91.209501	1196.267867	5.006938	-0.017575	1.987806
91.866607	1204.368260	5.011942	-0.017703	1.993634
92.094966	1212.468359	5.016947	-0.017751	1.999399
92.382858	1220.593395	5.021952	-0.017810	2.005172
92.626278	1228.712753	5.026957	-0.017860	2.010919
92.821832	1236.847734	5.031962	-0.017902	2.016656
93.334668	1244.933771	5.036966	-0.018003	2.022375
93.557256	1253.045225	5.041971	-0.018049	2.028065
94.251025	1261.153563	5.046976	-0.018184	2.033786
94.498930	1269.247404	5.051981	-0.018235	2.039435
94.973487	1277.315720	5.056986	-0.018329	2.045074
95.712228	1285.389667	5.061990	-0.018472	2.050727
96.032067	1293.507721	5.066995	-0.018536	2.056353
96.696932	1301.580743	5.072000	-0.018665	2.061968
96.878175	1309.706373	5.077005	-0.018704	2.067554
97.419462	1317.807555	5.082010	-0.018810	2.073145
97.751503	1325.908794	5.087014	-0.018878	2.078699
98.004318	1333.991772	5.092019	-0.018930	2.084219
98.631996	1342.066127	5.097024	-0.019052	2.089755
98.874818	1350.201375	5.102029	-0.019102	2.095279
99.305476	1358.278003	5.107034	-0.019188	2.100768
99.841049	1366.357667	5.112038	-0.019293	2.106255
100.232062	1374.486946	5.117043	-0.019371	2.111746
100.786248	1382.600606	5.122048	-0.019479	2.117229
101.145968	1390.666105	5.127053	-0.019552	2.122646
101.724048	1398.715670	5.132058	-0.019664	2.128060
102.244324	1406.820392	5.137062	-0.019767	2.133491
102.582273	1414.906742	5.142067	-0.019835	2.138878
103.023082	1422.993091	5.147072	-0.019922	2.144262
103.403957	1431.077383	5.152077	-0.019998	2.149625
103.808657	1439.181138	5.157082	-0.020079	2.154989
104.175625	1447.256441	5.162086	-0.020152	2.160318
104.312882	1455.346248	5.167091	-0.020183	2.165622
104.978323	1463.425128	5.172096	-0.020312	2.170955
105.313179	1471.530317	5.177101	-0.020380	2.176261
105.645973	1479.605531	5.182106	-0.020447	2.181534
106.186359	1487.681490	5.187110	-0.020553	2.186814
106.479072	1495.795272	5.192115	-0.020613	2.192083
107.052947	1503.867232	5.197120	-0.020725	2.197338
107.448877	1511.929628	5.202125	-0.020804	2.202558
107.892526	1519.996442	5.207130	-0.020892	2.207773
108.298541	1528.096511	5.212134	-0.020973	2.212993
108.668557	1536.167712	5.217139	-0.021047	2.218179
109.010545	1544.258092	5.222144	-0.021116	2.223363
109.590371	1552.304758	5.227149	-0.021229	2.228527
109.971158	1560.430927	5.232154	-0.021305	2.233713
110.399081	1568.490364	5.237158	-0.021390	2.238848
110.901845	1576.532915	5.242163	-0.021489	2.243968
111.170170	1584.649725	5.247168	-0.021544	2.249102
111.689226	1592.710077	5.252173	-0.021646	2.254210
112.211037	1600.775247	5.257178	-0.021748	2.259310
112.589020	1608.856747	5.262182	-0.021824	2.264396
112.646736	1616.979052	5.267187	-0.021840	2.269469
112.884770	1625.168429	5.272192	-0.021890	2.274587
113.143041	1633.195499	5.277197	-0.021943	2.279595
113.582004	1641.221775	5.282202	-0.022030	2.284607
113.677805	1649.325677	5.287206	-0.022053	2.289626
114.183655	1657.366181	5.292211	-0.022152	2.294630
114.557297	1665.421197	5.297216	-0.022227	2.299621
114.854382	1673.479562	5.302221	-0.022288	2.304597
114.820581	1681.601928	5.307226	-0.022287	2.309573
115.277994	1689.689902	5.312230	-0.022377	2.314558
115.737203	1697.691450	5.317235	-0.022468	2.319481
115.995911	1705.763853	5.322240	-0.022521	2.324419
116.346111	1713.826744	5.327245	-0.022592	2.329348
116.414780	1721.954035	5.332250	-0.022610	2.334283
116.929676	1729.990698	5.337254	-0.022711	2.339189
117.727165	1737.977012	5.342259	-0.022864	2.344077
118.112064	1746.081307	5.347264	-0.022941	2.348993
118.333182	1754.197205	5.352269	-0.022988	2.353891
118.533903	1762.264968	5.357274	-0.023030	2.358749
119.017602	1770.311076	5.362278	-0.023126	2.363607
119.095951	1778.397560	5.367283	-0.023146	2.368446
119.505455	1786.477850	5.372288	-0.023227	2.373299
120.070972	1794.497565	5.377293	-0.023338	2.378117
120.417228	1802.553079	5.382298	-0.023407	2.382930
120.906095	1810.634753	5.387302	-0.023504	2.387759
121.350152	1818.701083	5.392307	-0.023591	2.392567
122.052596	1826.746529	5.397312	-0.023727	2.397372
122.400920	1834.799055	5.402317	-0.023798	2.402144
122.613640	1842.866489	5.407322	-0.023842	2.406904
123.066909	1850.943096	5.412326	-0.023932	2.411680
123.304751	1859.022463	5.417331	-0.023982	2.416430
123.567419	1867.101240	5.422336	-0.024036	2.421173
123.637034	1875.179273	5.427341	-0.024054	2.425891
124.082242	1883.249484	5.432346	-0.024142	2.430625
124.462821	1891.382704	5.437350	-0.024218	2.435380
124.888819	1899.368765	5.442355	-0.024303	2.440045
125.464914	1907.371697	5.447360	-0.024415	2.444721
125.673404	1915.454041	5.452365	-0.024459	2.449407
126.049581	1923.527571	5.457370	-0.024534	2.454091
126.712345	1931.551553	5.462374	-0.024663	2.458759
126.976393	1939.591684	5.467379	-0.024717	2.463397
127.469649	1947.665451	5.472384	-0.024815	2.468064
127.769190	1955.737217	5.477389	-0.024876	2.472705
128.081238	1963.801933	5.482394	-0.024939	2.477335
128.421917	1971.860409	5.487398	-0.025008	2.481955
128.804291	1979.884782	5.492403	-0.025084	2.486549
129.147449	1987.979670	5.497408	-0.025153	2.491172
129.228842	1996.076021	5.502413	-0.025174	2.495769
129.648894	2004.088105	5.507418	-0.025257	2.500334
129.995780	2012.150544	5.512422	-0.025327	2.504913
130.174892	2020.232120	5.517427	-0.025365	2.509483
130.480214	2028.347295	5.522432	-0.025428	2.514072
130.696247	2036.389121	5.527437	-0.025473	2.518605
131.034316	2044.399841	5.532442	-0.025541	2.523122
131.426505	2052.441929	5.537446	-0.025619	2.527652
131.814317	2060.496181	5.542451	-0.025697	2.532180
132.124139	2068.571973	5.547456	-0.025760	2.536706
132.342355	2076.630007	5.552461	-0.025806	2.541208
132.543714	2084.668916	5.557466	-0.025848	2.545690
133.114326	2092.733787	5.562470	-0.025960	2.550204
133.461761	2100.781813	5.567475	-0.026030	2.554685
133.746023	2108.840043	5.572480	-0.026088	2.559160
133.881238	2116.899417	5.577485	-0.026118	2.563617
134.136289	2124.953806	5.582490	-0.026171	2.568072
134.286762	2133.036382	5.587494	-0.026204	2.572527
134.631988	2141.075543	5.592499	-0.026274	2.576964
135.098235	2149.100453	5.597504	-0.026366	2.581394
135.031595	2157.196319	5.602509	-0.026359	2.585818
135.393034	2165.251524	5.607514	-0.026431	2.590243
135.794814	2173.484184	5.612518	-0.026511	2.594758
136.046921	2181.447573	5.617523	-0.026563	2.599110
136.518733	2189.428122	5.622528	-0.026656	2.603478
136.964370	2197.428216	5.627533	-0.026745	2.607847
137.198641	2205.487610	5.632538	-0.026793	2.612227
137.578090	2213.543529	5.637542	-0.026869	2.616608
137.893480	2221.547883	5.642547	-0.026933	2.620949
138.154103	2229.611915	5.647552	-0.026987	2.625311
138.255395	2237.689166	5.652557	-0.027011	2.629662
138.545520	2245.748720	5.657562	-0.027070	2.634010
138.853036	2253.783494	5.662566	-0.027133	2.638338
139.092803	2261.806998	5.667571	-0.027183	2.642648
139.266502	2269.866773	5.672576	-0.027220	2.646966
139.736661	2277.892944	5.677581	-0.027313	2.651279
140.200426	2285.953492	5.682586	-0.027405	2.655602
140.562030	2293.995282	5.687590	-0.027477	2.659902
140.621542	2302.055369	5.692595	-0.027493	2.664184
141.266189	2310.076078	5.697600	-0.027619	2.668477
141.592457	2318.172418	5.702605	-0.027685	2.672782
141.883694	2326.209971	5.707610	-0.027744	2.677047
142.389406	2334.213204	5.712614	-0.027844	2.681301
142.673152	2342.250373	5.717619	-0.027902	2.685552
143.061751	2350.300262	5.722624	-0.027979	2.689809
143.203046	2358.407844	5.727629	-0.028011	2.694074
143.401185	2366.457138	5.732634	-0.028053	2.698305
143.784308	2374.488593	5.737638	-0.028129	2.702532
144.002637	2382.529307	5.742643	-0.028175	2.706747
144.265698	2390.585714	5.747648	-0.028229	2.710966
144.622127	2398.653861	5.752653	-0.028301	2.715190
144.750668	2406.681493	5.757658	-0.028330	2.719373
145.145450	2414.731342	5.762662	-0.028409	2.723577
145.298209	2422.767227	5.767667	-0.028443	2.727752
145.716196	2430.819010	5.772672	-0.028526	2.731946
145.850620	2438.909802	5.777677	-0.028556	2.736135
146.473895	2446.887363	5.782682	-0.028677	2.740290
146.835968	2454.930114	5.787686	-0.028750	2.744456
147.045155	2462.974198	5.792691	-0.028794	2.748607
147.526419	2471.090956	5.797696	-0.028889	2.752806
147.688551	2479.165955	5.802701	-0.028924	2.756957
147.917480	2487.161186	5.807706	-0.028972	2.761065
148.143042	2495.201239	5.812710	-0.029019	2.765190
148.374392	2503.204414	5.817715	-0.029068	2.769290
148.929646	2511.244850	5.822720	-0.029176	2.773422
149.214096	2519.297898	5.827725	-0.029234	2.777539
149.627041	2527.308140	5.832730	-0.029316	2.781635
150.100700	2535.344913	5.837734	-0.029410	2.785742
150.426324	2543.385733	5.842739	-0.029476	2.789836
150.771470	2551.470249	5.847744	-0.029545	2.793947
151.097186	2559.518423	5.852749	-0.029611	2.798033
151.269192	2567.538101	5.857754	-0.029648	2.802089
151.535014	2575.598991	5.862758	-0.029703	2.806166
151.911541	2583.602503	5.867763	-0.029778	2.810214
152.000367	2591.715518	5.872768	-0.029800	2.814295
152.129997	2599.765305	5.877773	-0.029830	2.818341
152.535271	2607.762734	5.882778	-0.029910	2.822370
152.800509	2615.829684	5.887782	-0.029965	2.826420
152.952658	2623.871229	5.892787	-0.029998	2.830445
153.234421	2631.958402	5.897792	-0.030056	2.834495
153.538575	2639.950626	5.902797	-0.030118	2.838493
153.859210	2647.961214	5.907802	-0.030183	2.842495
154.400577	2655.983416	5.912806	-0.030289	2.846509
154.775201	2664.002731	5.917811	-0.030364	2.850507
155.079370	2672.084377	5.922816	-0.030426	2.854527
155.243693	2680.143452	5.927821	-0.030461	2.858521
155.246979	2688.204825	5.932826	-0.030467	2.862502
155.662764	2696.227268	5.937830	-0.030550	2.866482
155.653085	2704.276474	5.942835	-0.030553	2.870445
156.212804	2712.317505	5.947840	-0.030663	2.874430
156.563726	2720.338644	5.952845	-0.030733	2.878389
156.635718	2728.381130	5.957850	-0.030752	2.882337
156.995001	2736.416079	5.962854	-0.030824	2.886291
157.754270	2744.397962	5.967859	-0.030971	2.890236
157.966355	2752.527403	5.972864	-0.031015	2.894218
158.222137	2760.552502	5.977869	-0.031068	2.898146
158.299741	2768.589743	5.982874	-0.031088	2.902065
158.793002	2776.620899	5.987878	-0.031185	2.905998
158.865714	2784.682555	5.992883	-0.031204	2.909917
159.030352	2792.823586	5.997888	-0.031240	2.913875
159.635710	2800.800321	6.002893	-0.031358	2.917771
159.990497	2808.765154	6.007898	-0.031429	2.921643
160.251119	2816.818308	6.012902	-0.031483	2.925548
160.212256	2824.837387	6.017907	-0.031481	2.929414
160.798631	2832.893520	6.022912	-0.031595	2.933327
160.997831	2840.924324	6.027917	-0.031637	2.937202
161.235773	2848.949283	6.032922	-0.031687	2.941070
161.576079	2856.986859	6.037926	-0.031755	2.944945
161.666514	2865.014683	6.042931	-0.031777	2.948798
161.991680	2873.089041	6.047936	-0.031843	2.952679
162.232542	2881.132978	6.052941	-0.031893	2.956537
162.525745	2889.143963	6.057946	-0.031953	2.960376
162.824677	2897.179966	6.062950	-0.032014	2.964223
163.053733	2905.220950	6.067955	-0.032062	2.968063
163.239536	2913.273167	6.072960	-0.032102	2.971902
163.406864	2921.341823	6.077965	-0.032138	2.975742
163.772918	2929.313505	6.082970	-0.032211	2.979542
164.163559	2937.371424	6.087974	-0.032289	2.983378
164.389645	2945.396673	6.092979	-0.032337	2.987186
164.539823	2953.477374	6.097984	-0.032370	2.991012
164.796229	2961.541362	6.102989	-0.032423	2.994829
165.070070	2969.519145	6.107994	-0.032479	2.998603
165.614456	2977.539633	6.112998	-0.032586	3.002405
165.873953	2985.558727	6.118003	-0.032639	3.006187
166.404117	2993.566919	6.123008	-0.032743	3.009973
166.574495	3001.669882	6.128013	-0.032780	3.013780
166.781845	3009.688587	6.133018	-0.032824	3.017545
167.269385	3017.711500	6.138022	-0.032920	3.021322
167.339828	3025.732738	6.143027	-0.032938	3.025072
167.546441	3033.808713	6.148032	-0.032982	3.028849
167.920882	3041.857991	6.153037	-0.033057	3.032618
168.011825	3049.912671	6.158042	-0.033079	3.036370
168.306274	3057.930746	6.163046	-0.033139	3.040111
168.588172	3065.927179	6.168051	-0.033197	3.043837
169.036327	3073.982435	6.173056	-0.033285	3.047593
168.940386	3082.074232	6.178061	-0.033273	3.051335
169.076818	3090.096641	6.183066	-0.033303	3.055052
169.412093	3098.123370	6.188070	-0.033371	3.058776
169.765345	3106.122331	6.193075	-0.033442	3.062483
169.922117	3114.175666	6.198080	-0.033476	3.066201
170.110104	3122.213958	6.203085	-0.033517	3.069909
170.436080	3130.318698	6.208090	-0.033582	3.073650
170.619983	3138.356071	6.213094	-0.033622	3.077349
170.996398	3146.331911	6.218099	-0.033697	3.081024
171.343070	3154.298658	6.223104	-0.033767	3.084688
171.713546	3162.350505	6.228109	-0.033841	3.088389
171.862442	3170.378493	6.233114	-0.033874	3.092064
172.299363	3178.432296	6.238118	-0.033961	3.095759
172.507034	3186.430580	6.243123	-0.034005	3.099415
172.915494	3194.449845	6.248128	-0.034086	3.103084
173.088902	3202.529135	6.253133	-0.034123	3.106766
173.191168	3210.582568	6.258138	-0.034148	3.110428
173.614744	3218.616963	6.263142	-0.034232	3.114092
173.724164	3226.617155	6.268147	-0.034257	3.117722
174.052218	3234.656097	6.273152	-0.034324	3.121375
174.335875	3242.655130	6.278157	-0.034382	3.125004
174.416172	3250.716242	6.283162	-0.034402	3.128648
175.181127	3258.742761	6.288166	-0.034549	3.132302
175.583340	3266.757920	6.293171	-0.034629	3.135930
175.778411	3274.785584	6.298176	-0.034671	3.139551
176.090380	3282.835476	6.303181	-0.034734	3.143182
176.388562	3290.853743	6.308186	-0.034795	3.146794
176.734981	3298.922648	6.313190	-0.034865	3.150428
176.794648	3306.994843	6.318195	-0.034881	3.154045
177.421995	3314.995243	6.323200	-0.035003	3.157652
177.810224	3323.008766	6.328205	-0.035081	3.161249
177.715566	3331.014748	6.333210	-0.035068	3.164818
177.974658	3339.052253	6.338214	-0.035122	3.168412
178.117188	3347.136233	6.343219	-0.035153	3.172018
178.432365	3355.145431	6.348224	-0.035217	3.175594
178.716251	3363.187221	6.353229	-0.035275	3.179179
179.055545	3371.177310	6.358234	-0.035344	3.182740
179.359903	3379.246110	6.363238	-0.035406	3.186329
179.447463	3387.275754	6.368243	-0.035427	3.189888
179.846328	3395.308025	6.373248	-0.035507	3.193458
179.937778	3403.390068	6.378253	-0.035529	3.197032
180.282475	3411.344599	6.383258	-0.035598	3.200557
180.422416	3419.363629	6.388262	-0.035630	3.204098
180.987876	3427.407390	6.393267	-0.035740	3.207663
181.239435	3435.463748	6.398272	-0.035792	3.211217
181.348871	3443.523357	6.403277	-0.035818	3.214762
181.592876	3451.537274	6.408282	-0.035868	3.218289
181.948770	3459.563862	6.413286	-0.035940	3.221822
182.357564	3467.528858	6.418291	-0.036021	3.225327
182.370316	3475.610435	6.423296	-0.036029	3.228862
182.716575	3483.687658	6.428301	-0.036098	3.232405
183.055197	3491.727393	6.433306	-0.036167	3.235928
183.270664	3499.728743	6.438310	-0.036212	3.239425
183.583363	3507.719800	6.443315	-0.036275	3.242917
183.684127	3515.764361	6.448320	-0.036299	3.246421
183.744152	3523.809208	6.453325	-0.036316	3.249919
183.996310	3531.829235	6.458330	-0.036368	3.253410
184.418820	3539.872612	6.463334	-0.036452	3.256915
184.536575	3547.882854	6.468339	-0.036479	3.260389
184.888900	3555.892515	6.473344	-0.036550	3.263868
185.327038	3563.935591	6.478349	-0.036637	3.267362
185.257275	3571.969375	6.483354	-0.036629	3.270828
185.476763	3580.034608	6.488358	-0.036675	3.274315
185.798828	3588.014416	6.493363	-0.036740	3.277765
186.159942	3596.020310	6.498368	-0.036813	3.281224
186.378953	3604.057116	6.503373	-0.036859	3.284688
186.508614	3612.090205	6.508378	-0.036888	3.288143
186.849802	3620.171768	6.513382	-0.036957	3.291623
187.002088	3628.196642	6.518387	-0.036990	3.295068
187.433115	3636.186793	6.523392	-0.037076	3.298505
187.870409	3644.235334	6.528397	-0.037162	3.301963
188.009855	3652.215984	6.533402	-0.037193	3.305378
188.462160	3660.272287	6.538406	-0.037283	3.308833
188.795461	3668.308963	6.543411	-0.037350	3.312272
189.078747	3676.365191	6.548416	-0.037408	3.315713
189.242517	3684.380282	6.553421	-0.037444	3.319129
189.513429	3692.375158	6.558426	-0.037499	3.322536
189.757841	3700.418971	6.563430	-0.037550	3.325960
189.779828	3708.444320	6.568435	-0.037560	3.329365
190.102753	3716.489144	6.573440	-0.037625	3.332785
190.599398	3724.519093	6.578445	-0.037723	3.336201
190.471414	3732.532931	6.583450	-0.037704	3.339585
190.643999	3740.600430	6.588454	-0.037741	3.342998
190.952563	3748.597830	6.593459	-0.037804	3.346384
191.472604	3756.608880	6.598464	-0.037906	3.349779
191.730125	3764.683644	6.603469	-0.037959	3.353189
191.785412	3772.719585	6.608474	-0.037975	3.356571
192.254965	3780.705725	6.613478	-0.038067	3.359943
192.377356	3788.727685	6.618483	-0.038095	3.363315
192.502415	3796.762001	6.623488	-0.038124	3.366689
193.044874	3804.801586	6.628493	-0.038230	3.370076
193.180435	3812.863314	6.633498	-0.038260	3.373455
193.468984	3820.879091	6.638502	-0.038319	3.376816
193.655466	3828.879501	6.643507	-0.038359	3.380164
193.796772	3836.923955	6.648512	-0.038391	3.383526
194.193484	3844.961653	6.653517	-0.038470	3.386890
194.274037	3852.971921	6.658522	-0.038490	3.390228
194.608970	3861.111408	6.663526	-0.038558	3.393626
194.767656	3869.122925	6.668531	-0.038593	3.396961
194.928480	3877.081278	6.673536	-0.038628	3.400271
195.390823	3885.080280	6.678541	-0.038719	3.403604
195.510256	3893.075205	6.683546	-0.038746	3.406921
195.623751	3901.135071	6.688550	-0.038773	3.410261
195.790074	3909.176616	6.693555	-0.038809	3.413592
196.301106	3917.164323	6.698560	-0.038909	3.416910
196.591774	3925.169898	6.703565	-0.038969	3.420224
196.878572	3933.188245	6.708570	-0.039027	3.423540
197.208397	3941.245097	6.713574	-0.039094	3.426870
197.263604	3949.281593	6.718579	-0.039109	3.430179
197.515102	3957.318195	6.723584	-0.039161	3.433491
197.748288	3965.373303	6.728589	-0.039210	3.436807
198.001349	3973.348670	6.733594	-0.039262	3.440088
198.316659	3981.398349	6.738598	-0.039326	3.443398
198.401261	3989.419692	6.743603	-0.039347	3.446686
198.562595	3997.415823	6.748608	-0.039382	3.449963
198.861776	4005.500232	6.753613	-0.039443	3.453277
198.815692	4013.565231	6.758618	-0.039440	3.456569
199.208040	4021.566002	6.763622	-0.039518	3.459846
199.506111	4029.548367	6.768627	-0.039579	3.463109
199.660832	4037.577460	6.773632	-0.039613	3.466384
199.901634	4045.627335	6.778637	-0.039663	3.469666
200.191976	4053.681019	6.783642	-0.039722	3.472949
200.483292	4061.714694	6.788646	-0.039782	3.476220
200.831372	4069.664582	6.793651	-0.039852	3.479456
201.008825	4077.688667	6.798656	-0.039890	3.482713
201.442860	4085.728725	6.803661	-0.039976	3.485982
201.687216	4093.721145	6.808666	-0.040027	3.489223
201.977129	4101.777839	6.813670	-0.040086	3.492488
202.055107	4109.831673	6.818675	-0.040106	3.495742
202.294307	4117.781387	6.823680	-0.040155	3.498956
202.569046	4125.839630	6.828685	-0.040212	3.502212
202.824302	4133.865120	6.833690	-0.040265	3.505451
202.932474	4141.900202	6.838694	-0.040290	3.508686
202.981694	4149.951964	6.843699	-0.040304	3.511924
203.183600	4157.991669	6.848704	-0.040347	3.515158
203.541850	4165.988736	6.853709	-0.040419	3.518377
203.471166	4174.023762	6.858714	-0.040411	3.521594
203.776125	4182.025756	6.863718	-0.040473	3.524808
203.966605	4190.043908	6.868723	-0.040514	3.528021
204.222259	4198.079368	6.873728	-0.040566	3.531240
204.438152	4206.146416	6.878733	-0.040612	3.534467
204.531545	4214.159724	6.883738	-0.040635	3.537667
204.772033	4222.198255	6.888742	-0.040684	3.540878
205.141614	4230.176459	6.893747	-0.040758	3.544066
205.619332	4238.213590	6.898752	-0.040853	3.547277
205.790438	4246.277211	6.903757	-0.040890	3.550487
205.773191	4254.392927	6.908762	-0.040892	3.553709
205.967460	4262.387707	6.913766	-0.040933	3.556887
206.399513	4270.346890	6.918771	-0.041019	3.560055
206.347599	4278.352302	6.923776	-0.041014	3.563223
206.865025	4286.399410	6.928781	-0.041116	3.566423
206.919605	4294.382943	6.933786	-0.041131	3.569580
207.172252	4302.442874	6.938790	-0.041183	3.572771
207.323490	4310.460562	6.943795	-0.041217	3.575939
207.495380	4318.445902	6.948800	-0.041254	3.579092
207.756708	4326.488159	6.953805	-0.041308	3.582268
207.883152	4334.497467	6.958810	-0.041337	3.585423
208.288746	4342.504812	6.963814	-0.041417	3.588583
208.256087	4350.585227	6.968819	-0.041417	3.591757
208.612112	4358.577958	6.973824	-0.041488	3.594904
208.874899	4366.607652	6.978829	-0.041542	3.598061
209.108972	4374.607518	6.983834	-0.041591	3.601202
209.531258	4382.591469	6.988838	-0.041675	3.604339
209.911337	4390.654254	6.993843	-0.041751	3.607503
210.207800	4398.647113	6.998848	-0.041811	3.610635
210.340861	4406.730619	7.003853	-0.041841	3.613795
210.540170	4414.763745	7.008858	-0.041884	3.616934
211.004771	4422.716347	7.013862	-0.041975	3.620046
211.173799	4430.785795	7.018867	-0.042012	3.623193
211.333274	4438.807620	7.023872	-0.042047	3.626319
211.777797	4446.811717	7.028877	-0.042135	3.629442
212.166065	4454.892775	7.033882	-0.042212	3.632591
212.346209	4462.926264	7.038886	-0.042251	3.635714
212.487649	4470.913843	7.043891	-0.042283	3.638814
212.905754	4478.931931	7.048896	-0.042366	3.641932
213.080627	4486.929451	7.053901	-0.042403	3.645032
213.054178	4494.975956	7.058906	-0.042404	3.648143
213.329544	4503.023209	7.063910	-0.042460	3.651260
213.725669	4511.044953	7.068915	-0.042539	3.654367
213.774091	4519.066612	7.073920	-0.042553	3.657462
213.873952	4527.125641	7.078925	-0.042577	3.660571
213.962991	4535.095784	7.083930	-0.042599	3.663642
214.264131	4543.137087	7.088934	-0.042660	3.666744
214.478774	4551.152977	7.093939	-0.042705	3.669831
214.886209	4559.173351	7.098944	-0.042786	3.672922
215.162650	4567.242805	7.103949	-0.042843	3.676026
215.122575	4575.218961	7.108954	-0.042841	3.679083
215.189620	4583.275320	7.113958	-0.042859	3.682172
215.651794	4591.262501	7.118963	-0.042950	3.685241
215.668264	4599.262349	7.123968	-0.042958	3.688301
216.058737	4607.330824	7.128973	-0.043036	3.691394
216.255284	4615.356014	7.133978	-0.043078	3.694464
216.511752	4623.387320	7.138982	-0.043131	3.697534
216.490742	4631.399312	7.143987	-0.043132	3.700588
216.614660	4639.366655	7.148992	-0.043160	3.703626
217.074219	4647.404969	7.153997	-0.043251	3.706696
217.076622	4655.449378	7.159002	-0.043257	3.709755
217.258370	4663.571060	7.164006	-0.043296	3.712845
217.504614	4671.596714	7.169011	-0.043347	3.715898
217.872939	4679.525731	7.174016	-0.043421	3.718914
217.884962	4687.606121	7.179021	-0.043428	3.721977
218.177167	4695.531793	7.184026	-0.043488	3.724985
218.552536	4703.581710	7.189030	-0.043563	3.728040
218.819803	4711.626257	7.194035	-0.043618	3.731088
218.898715	4719.653033	7.199040	-0.043638	3.734122
219.098934	4727.699421	7.204045	-0.043680	3.737164
219.197174	4735.667768	7.209050	-0.043704	3.740171
219.359654	4743.695746	7.214054	-0.043739	3.743200
219.777583	4751.704402	7.219059	-0.043822	3.746225
219.982857	4759.713863	7.224064	-0.043866	3.749243
219.998402	4767.813101	7.229069	-0.043874	3.752288
220.088123	4775.827864	7.234074	-0.043896	3.755301
220.428832	4783.817823	7.239078	-0.043964	3.758307
220.689433	4791.858405	7.244083	-0.044018	3.761328
220.678125	4799.815536	7.249088	-0.044021	3.764309
221.022992	4807.889866	7.254093	-0.044091	3.767340
221.265072	4815.870248	7.259098	-0.044141	3.770331
221.265108	4823.931926	7.264102	-0.044146	3.773345
221.542657	4831.980763	7.269107	-0.044203	3.776357
221.781367	4839.958153	7.274112	-0.044253	3.779339
222.007842	4848.033150	7.279117	-0.044300	3.782356
222.150171	4855.994840	7.284122	-0.044332	3.785325
222.455921	4864.040341	7.289126	-0.044394	3.788327
222.553860	4872.094656	7.294131	-0.044417	3.791326
222.586560	4880.143302	7.299136	-0.044429	3.794318
223.051178	4888.135789	7.304141	-0.044520	3.797297
223.213777	4896.099538	7.309146	-0.044556	3.800256
223.348000	4904.139459	7.314150	-0.044586	3.803240
223.626483	4912.108198	7.319155	-0.044643	3.806199
223.836524	4920.155587	7.324160	-0.044687	3.809183
224.017758	4928.214437	7.329165	-0.044726	3.812168
224.085496	4936.237263	7.334170	-0.044744	3.815135
224.560165	4944.217503	7.339174	-0.044838	3.818093
224.681540	4952.275252	7.344179	-0.044865	3.821070
224.729668	4960.257165	7.349184	-0.044880	3.824014
225.086959	4968.314879	7.354189	-0.044951	3.826991
225.354534	4976.286597	7.359194	-0.045006	3.829932
225.435515	4984.358349	7.364198	-0.045027	3.832904
225.359366	4992.397725	7.369203	-0.045018	3.835858
225.634733	5000.358837	7.374208	-0.045074	3.838788
225.818330	5008.438519	7.379213	-0.045114	3.841758
225.837806	5016.388126	7.384218	-0.045122	3.844674
226.309710	5024.447209	7.389222	-0.045215	3.847637
226.585274	5032.441766	7.394227	-0.045272	3.850571
226.742252	5040.507152	7.399232	-0.045306	3.853525
227.206122	5048.563566	7.404237	-0.045398	3.856481
227.406375	5056.533170	7.409242	-0.045441	3.859397
227.435953	5064.597809	7.414246	-0.045451	3.862342
227.752705	5072.553626	7.419251	-0.045515	3.865250
228.163862	5080.610678	7.424256	-0.045597	3.868196
228.387876	5088.685066	7.429261	-0.045644	3.871141
228.404338	5096.919365	7.434266	-0.045653	3.874139
228.668393	5104.878799	7.439270	-0.045707	3.877039
229.212478	5112.771709	7.444275	-0.045813	3.879918
229.207050	5120.740520	7.449280	-0.045817	3.882812
229.411890	5128.739367	7.454285	-0.045861	3.885718
229.747555	5136.763193	7.459290	-0.045929	3.888634
229.847594	5144.809102	7.464294	-0.045952	3.891551
230.011370	5152.848251	7.469299	-0.045988	3.894465
230.285401	5160.809154	7.474304	-0.046044	3.897351
230.515366	5168.852681	7.479309	-0.046092	3.900263
230.644116	5176.861777	7.484314	-0.046121	3.903158
231.064170	5184.869550	7.489318	-0.046205	3.906057
231.322601	5192.938572	7.494323	-0.046258	3.908972
231.381151	5200.921785	7.499328	-0.046274	3.911851
231.602596	5208.989265	7.504333	-0.046321	3.914760
231.926939	5216.962131	7.509338	-0.046386	3.917636
232.146472	5224.961969	7.514342	-0.046432	3.920517
232.342712	5232.955069	7.519347	-0.046474	3.923393
232.495077	5240.991131	7.524352	-0.046508	3.926281
232.904442	5249.043745	7.529357	-0.046589	3.929178
232.760742	5257.071861	7.534362	-0.046568	3.932054
232.972979	5265.120271	7.539366	-0.046612	3.934942
233.469905	5273.118655	7.544371	-0.046710	3.937814
233.277804	5281.112729	7.549376	-0.046680	3.940671
233.671815	5289.083592	7.554381	-0.046758	3.943527
233.694054	5297.126774	7.559386	-0.046767	3.946401
233.945137	5305.147129	7.564390	-0.046819	3.949269
234.159316	5313.232135	7.569395	-0.046865	3.952157
234.403760	5321.233192	7.574400	-0.046915	3.955013
234.692984	5329.269542	7.579405	-0.046974	3.957881
234.902241	5337.211290	7.584410	-0.047018	3.960711
235.084670	5345.235616	7.589414	-0.047058	3.963568
235.205483	5353.296880	7.594419	-0.047085	3.966435
235.369894	5361.281941	7.599424	-0.047121	3.969274
235.830049	5369.322128	7.604429	-0.047212	3.972136
235.944338	5377.345902	7.609434	-0.047238	3.974983
236.151425	5385.391390	7.614438	-0.047282	3.977838
236.399065	5393.377357	7.619443	-0.047334	3.980670
236.776009	5401.396629	7.624448	-0.047409	3.983514
237.312846	5409.429387	7.629453	-0.047514	3.986364
237.628397	5417.428868	7.634458	-0.047578	3.989196
237.756229	5425.490578	7.639462	-0.047607	3.992045
237.961926	5433.528872	7.644467	-0.047651	3.994884
237.990475	5441.550953	7.649472	-0.047661	3.997714
238.227969	5449.561260	7.654477	-0.047711	4.000540
238.384602	5457.560599	7.659482	-0.047745	4.003359
238.763608	5465.567165	7.664486	-0.047821	4.006182
238.717211	5473.594198	7.669491	-0.047817	4.009004
238.934184	5481.629325	7.674496	-0.047863	4.011831
239.318843	5489.682327	7.679501	-0.047940	4.014664
239.286511	5497.695570	7.684506	-0.047939	4.017475
239.460826	5505.695508	7.689510	-0.047977	4.020283
239.794339	5513.712847	7.694515	-0.048044	4.023097
239.991156	5521.713378	7.699520	-0.048086	4.025901
240.151058	5529.766707	7.704525	-0.048121	4.028721
240.288339	5537.778499	7.709530	-0.048151	4.031525
240.492298	5545.886913	7.714534	-0.048195	4.034361
240.756501	5553.916245	7.719539	-0.048249	4.037168
240.945468	5561.816648	7.724544	-0.048289	4.039927
241.240430	5569.882847	7.729549	-0.048350	4.042744
241.421850	5577.828738	7.734554	-0.048389	4.045515
241.289307	5585.865155	7.739558	-0.048369	4.048311
241.523267	5593.889907	7.744563	-0.048418	4.051106
241.630648	5601.933677	7.749568	-0.048443	4.053905
241.854316	5609.987212	7.754573	-0.048490	4.056706
241.895155	5617.933447	7.759578	-0.048503	4.059466
242.258931	5625.957324	7.764582	-0.048576	4.062255
242.503469	5633.983656	7.769587	-0.048626	4.065041
242.481498	5641.963380	7.774592	-0.048627	4.067806
242.851048	5649.999383	7.779597	-0.048701	4.070593
243.048514	5658.068768	7.784602	-0.048743	4.073388
243.308401	5666.066308	7.789606	-0.048797	4.076157
243.240127	5674.078916	7.794611	-0.048790	4.078925
243.400238	5682.072475	7.799616	-0.048825	4.081687
243.493543	5690.081411	7.804621	-0.048847	4.084452
244.056626	5698.085448	7.809626	-0.048957	4.087219
244.332463	5706.091921	7.814630	-0.049014	4.089982
244.520497	5714.139099	7.819635	-0.049054	4.092756
244.469384	5722.203834	7.824640	-0.049050	4.095530
244.969740	5730.202762	7.829645	-0.049148	4.098288
245.020044	5738.221871	7.834650	-0.049163	4.101044
245.165848	5746.253662	7.839654	-0.049195	4.103804
245.389893	5754.274300	7.844659	-0.049242	4.106560
245.763491	5762.253784	7.849664	-0.049317	4.109301
246.051833	5770.354967	7.854669	-0.049376	4.112081
246.180543	5778.382937	7.859674	-0.049405	4.114832
246.625090	5786.399091	7.864678	-0.049493	4.117582
246.719293	5794.360738	7.869683	-0.049515	4.120306
246.823535	5802.358395	7.874688	-0.049540	4.123041
246.900148	5810.398086	7.879693	-0.049560	4.125788
247.097123	5818.405844	7.884698	-0.049601	4.128524
247.217580	5826.426357	7.889702	-0.049629	4.131261
247.604757	5834.478346	7.894707	-0.049706	4.134011
247.663273	5842.516497	7.899712	-0.049722	4.136749
247.715454	5850.500603	7.904717	-0.049737	4.139468
248.008679	5858.546600	7.909722	-0.049797	4.142209
247.987569	5866.534755	7.914726	-0.049798	4.144924
248.188795	5874.592951	7.919731	-0.049841	4.147665
248.361703	5882.590410	7.924736	-0.049879	4.150382
248.531826	5890.650351	7.929741	-0.049915	4.153119
248.924449	5898.658263	7.934746	-0.049994	4.155839
249.000201	5906.644689	7.939750	-0.050013	4.158546
249.246301	5914.673884	7.944755	-0.050064	4.161267
249.433406	5922.627391	7.949760	-0.050104	4.163961
249.569945	5930.708813	7.954765	-0.050135	4.166696
249.742241	5938.724178	7.959770	-0.050172	4.169407
250.151572	5946.719356	7.964774	-0.050253	4.172111
250.604042	5954.776760	7.969779	-0.050343	4.174836
250.747321	5962.744269	7.974784	-0.050375	4.177525
250.977460	5970.775278	7.979789	-0.050423	4.180235
250.899301	5978.782712	7.984794	-0.050413	4.182931
251.208085	5986.784604	7.989798	-0.050476	4.185628
251.451224	5994.844035	7.994803	-0.050527	4.188342
251.467469	6002.848253	7.999808	-0.050535	4.191033
251.839303	6010.987604	8.004813	-0.050609	4.193772
251.885947	6018.981806	8.009818	-0.050623	4.196456
252.046094	6026.882651	8.014822	-0.050658	4.199109
252.351103	6034.945159	8.019827	-0.050720	4.201816
252.652220	6042.869601	8.024832	-0.050781	4.204475
252.797810	6050.940136	8.029837	-0.050814	4.207179
252.934797	6058.938744	8.034842	-0.050844	4.209857
253.114660	6066.977620	8.039846	-0.050883	4.212548
253.387047	6075.033865	8.044851	-0.050939	4.215243
253.546650	6083.000608	8.049856	-0.050974	4.217906
253.759698	6091.026994	8.054861	-0.051019	4.220588
253.842872	6099.055880	8.059866	-0.051040	4.223267
254.195951	6107.044479	8.064870	-0.051111	4.225934
254.486762	6115.069156	8.069875	-0.051170	4.228610
254.518246	6123.098147	8.074880	-0.051181	4.231284
254.756108	6131.145982	8.079885	-0.051230	4.233964
254.857235	6139.180407	8.084890	-0.051255	4.236637
255.176533	6147.127279	8.089894	-0.051319	4.239281
255.455332	6155.170667	8.094899	-0.051376	4.241955
255.504211	6163.140093	8.099904	-0.051391	4.244601
255.730607	6171.237607	8.104909	-0.051438	4.247289
255.745616	6179.168153	8.109914	-0.051446	4.249918
256.030915	6187.270580	8.114918	-0.051504	4.252604
256.387255	6195.285756	8.119923	-0.051576	4.255261
256.333626	6203.313446	8.124928	-0.051571	4.257917
256.679745	6211.299470	8.129933	-0.051641	4.260561
257.034249	6219.337633	8.134938	-0.051712	4.263220
257.217155	6227.330673	8.139942	-0.051751	4.265861
257.457194	6235.392536	8.144947	-0.051801	4.268524
257.665272	6243.394094	8.149952	-0.051845	4.271165
258.022504	6251.476409	8.154957	-0.051917	4.273832
258.034706	6259.497922	8.159962	-0.051924	4.276474
258.265597	6267.411619	8.164966	-0.051972	4.279082
258.539444	6275.484824	8.169971	-0.052029	4.281740
258.864733	6283.419397	8.174976	-0.052094	4.284351
258.790435	6291.536209	8.179981	-0.052086	4.287018
258.939520	6299.476577	8.184986	-0.052119	4.289627
259.161958	6307.544699	8.189990	-0.052165	4.292276
259.533344	6315.572372	8.194995	-0.052240	4.294912
259.511114	6323.573697	8.200000	-0.052241	4.297535
259.732981	6331.573092	8.205005	-0.052287	4.300157
259.828573	6339.624355	8.210010	-0.052310	4.302793
260.068717	6347.618961	8.215014	-0.052360	4.305411
260.264047	6355.654926	8.220019	-0.052402	4.308040
260.104765	6363.636274	8.225024	-0.052377	4.310647
260.243655	6371.719759	8.230029	-0.052408	4.313288
260.758905	6379.692491	8.235034	-0.052509	4.315894
261.052208	6387.701137	8.240038	-0.052569	4.318508
261.288870	6395.739985	8.245043	-0.052619	4.321130
261.369742	6403.685673	8.250048	-0.052639	4.323719
261.667751	6411.794437	8.255053	-0.052700	4.326361
261.615978	6419.755651	8.260058	-0.052695	4.328951
261.804665	6427.758662	8.265062	-0.052735	4.331555
262.240143	6435.850639	8.270067	-0.052822	4.334188
262.333788	6443.814611	8.275072	-0.052844	4.336775
262.569735	6451.825602	8.280077	-0.052893	4.339377
262.877351	6459.876588	8.285082	-0.052956	4.341991
263.112488	6467.827131	8.290086	-0.053005	4.344570
263.359948	6475.871888	8.295091	-0.053056	4.347178
263.483647	6483.901916	8.300096	-0.053084	4.349779
263.774094	6491.985564	8.305101	-0.053144	4.352397
263.690619	6500.044960	8.310106	-0.053133	4.355003
263.985887	6508.031152	8.315110	-0.053194	4.357586
264.127458	6515.992339	8.320115	-0.053225	4.360158
264.174598	6523.957217	8.325120	-0.053239	4.362730
264.450786	6531.967927	8.330125	-0.053296	4.365316
264.690180	6540.004543	8.335130	-0.053346	4.367909
264.848050	6548.039814	8.340134	-0.053380	4.370499
265.007211	6556.065353	8.345139	-0.053415	4.373085
265.080713	6564.050715	8.350144	-0.053434	4.375656
265.418441	6572.091345	8.355149	-0.053502	4.378244
265.665718	6580.098675	8.360154	-0.053553	4.380820
265.579884	6588.106055	8.365158	-0.053542	4.383392
265.818438	6596.105598	8.370163	-0.053592	4.385962
266.043587	6604.140337	8.375168	-0.053639	4.388542
266.079687	6612.220154	8.380173	-0.053651	4.391133
266.203936	6620.220452	8.385178	-0.053679	4.393698
266.571549	6628.240889	8.390182	-0.053753	4.396270
266.639434	6636.229212	8.395187	-0.053771	4.398828
266.867948	6644.238126	8.400192	-0.053819	4.401391
267.170537	6652.213496	8.405197	-0.053880	4.403943
267.191633	6660.253830	8.410202	-0.053889	4.406513
267.271714	6668.238298	8.415206	-0.053909	4.409064
267.614130	6676.331917	8.420211	-0.053978	4.411649
267.766676	6684.346241	8.425216	-0.054012	4.414207
268.099950	6692.387012	8.430221	-0.054079	4.416772
268.262640	6700.377344	8.435226	-0.054115	4.419319
268.443637	6708.391698	8.440230	-0.054154	4.421872
268.579747	6716.356476	8.445235	-0.054184	4.424408
268.695637	6724.424351	8.450240	-0.054211	4.426975
269.003584	6732.433317	8.455245	-0.054274	4.429522
269.098658	6740.490320	8.460250	-0.054297	4.432082
269.349939	6748.506587	8.465254	-0.054349	4.434629
269.589764	6756.562167	8.470259	-0.054398	4.437187
269.631345	6764.483390	8.475264	-0.054411	4.439699
269.676470	6772.559806	8.480269	-0.054425	4.442260
270.033485	6780.486989	8.485274	-0.054497	4.444772
270.361639	6788.538522	8.490278	-0.054563	4.447323
270.628899	6796.555127	8.495283	-0.054618	4.449861
270.566345	6804.610175	8.500288	-0.054611	4.452408
270.818385	6812.611601	8.505293	-0.054664	4.454938
270.944958	6820.658748	8.510298	-0.054692	4.457481
270.982403	6828.616653	8.515302	-0.054704	4.459994
271.495994	6836.651665	8.520307	-0.054805	4.462531
271.596478	6844.652658	8.525312	-0.054829	4.465054
271.686199	6852.719779	8.530317	-0.054851	4.467597
271.880935	6860.716012	8.535322	-0.054893	4.470117
272.124606	6868.713329	8.540326	-0.054943	4.472635
272.578700	6876.778501	8.545331	-0.055033	4.475174
272.724905	6884.725569	8.550336	-0.055065	4.477674
272.855941	6892.747851	8.555341	-0.055095	4.480195
273.356922	6900.777906	8.560346	-0.055193	4.482719
273.419542	6908.743453	8.565351	-0.055210	4.485220
273.519732	6916.798711	8.570355	-0.055234	4.487747
273.599301	6924.801988	8.575360	-0.055254	4.490257
273.952812	6932.832119	8.580365	-0.055325	4.492775
274.088568	6940.882864	8.585370	-0.055356	4.495297
274.364472	6948.885054	8.590375	-0.055412	4.497803
274.410427	6956.903830	8.595379	-0.055426	4.500311
274.570754	6964.858206	8.600384	-0.055461	4.502799
274.693527	6972.898311	8.605389	-0.055489	4.505312
274.888372	6980.938369	8.610394	-0.055531	4.507824
274.966657	6988.926907	8.615399	-0.055550	4.510317
275.362687	6997.054551	8.620403	-0.055629	4.512854
275.474650	7005.046881	8.625408	-0.055655	4.515346
275.520935	7013.031141	8.630413	-0.055669	4.517835
275.467812	7021.011525	8.635418	-0.055665	4.520320
275.805814	7028.996536	8.640423	-0.055733	4.522806
276.020146	7037.045150	8.645427	-0.055778	4.525311
276.036509	7045.038370	8.650432	-0.055786	4.527796
276.304707	7053.056473	8.655437	-0.055841	4.530289
276.509222	7061.110674	8.660442	-0.055884	4.532790
276.530208	7069.100109	8.665447	-0.055894	4.535271
276.557316	7077.122081	8.670451	-0.055904	4.537759
276.992038	7085.070619	8.675456	-0.055990	4.540225
277.172663	7093.138921	8.680461	-0.056029	4.542726
277.415421	7101.127735	8.685466	-0.056079	4.545200
277.706237	7109.173217	8.690471	-0.056139	4.547691
277.907016	7117.209544	8.695475	-0.056181	4.550178
277.893133	7125.221069	8.700480	-0.056184	4.552655
278.173782	7133.244722	8.705485	-0.056241	4.555136
278.564783	7141.289575	8.710490	-0.056319	4.557621
278.483703	7149.218532	8.715495	-0.056309	4.560069
278.708482	7157.343835	8.720499	-0.056356	4.562576
278.965294	7165.261932	8.725504	-0.056409	4.565018
279.119474	7173.363071	8.730509	-0.056443	4.567515
279.288295	7181.308483	8.735514	-0.056480	4.569963
279.198363	7189.378737	8.740519	-0.056468	4.572447
279.715700	7197.414002	8.745523	-0.056570	4.574920
279.652411	7205.416846	8.750528	-0.056563	4.577381
279.797786	7213.376706	8.755533	-0.056596	4.579828
280.145113	7221.436978	8.760538	-0.056666	4.582304
280.288320	7229.402524	8.765543	-0.056697	4.584750
280.487769	7237.511694	8.770547	-0.056740	4.587239
280.834345	7245.434684	8.775552	-0.056809	4.589669
281.000403	7253.495762	8.780557	-0.056846	4.592140
281.246811	7261.541774	8.785562	-0.056897	4.594605
281.273668	7269.545563	8.790567	-0.056907	4.597056
281.784270	7277.543968	8.795571	-0.057007	4.599504
281.781434	7285.588099	8.800576	-0.057012	4.601964
281.945151	7293.516920	8.805581	-0.057047	4.604388
282.082450	7301.613532	8.810586	-0.057078	4.606862
282.382713	7309.572376	8.815591	-0.057139	4.609292
282.375275	7317.621502	8.820595	-0.057143	4.611749
282.699603	7325.643242	8.825600	-0.057209	4.614196
282.907907	7333.670358	8.830605	-0.057253	4.616643
283.309838	7341.653763	8.835610	-0.057333	4.619076
283.382440	7349.679233	8.840615	-0.057352	4.621520
283.596036	7357.676291	8.845619	-0.057396	4.623955
283.500129	7365.701939	8.850624	-0.057384	4.626396
283.787213	7373.691225	8.855629	-0.057442	4.628825
283.969443	7381.787422	8.860634	-0.057482	4.631286
284.089200	7389.768637	8.865639	-0.057509	4.633710
284.171573	7397.816762	8.870643	-0.057530	4.636153
284.366797	7405.763404	8.875648	-0.057571	4.638565
284.464838	7413.803625	8.880653	-0.057595	4.641003
284.809355	7421.768376	8.885658	-0.057664	4.643417
284.791240	7429.799315	8.890663	-0.057666	4.645850
284.985967	7437.850550	8.895667	-0.057707	4.648287
285.155931	7445.835849	8.900672	-0.057744	4.650704
285.150441	7453.889844	8.905677	-0.057748	4.653140
285.323286	7461.875343	8.910682	-0.057786	4.655554
285.472535	7469.888745	8.915687	-0.057819	4.657975
285.653428	7477.917878	8.920691	-0.057858	4.660400
285.850014	7485.961681	8.925696	-0.057899	4.662827
286.145579	7493.930474	8.930701	-0.057960	4.665231
286.331726	7501.993117	8.935706	-0.058000	4.667662
286.607563	7509.962017	8.940711	-0.058056	4.670063
286.815768	7518.106912	8.945715	-0.058100	4.672516
287.019040	7526.111962	8.950720	-0.058143	4.674925
287.184380	7534.063946	8.955725	-0.058179	4.677318
287.095213	7542.005195	8.960730	-0.058168	4.679706
287.359968	7550.049082	8.965735	-0.058222	4.682123
287.575962	7557.997162	8.970739	-0.058268	4.684511
287.650349	7566.088940	8.975744	-0.058287	4.686940
287.972051	7574.067864	8.980749	-0.058352	4.689334
288.312894	7582.109420	8.985754	-0.058420	4.691746
288.220359	7590.114898	8.990759	-0.058408	4.694146
288.293912	7598.220410	8.995763	-0.058427	4.696575
288.460319	7606.144156	9.000768	-0.058463	4.698947
288.536840	7614.157923	9.005773	-0.058483	4.701346
288.698892	7622.180625	9.010778	-0.058518	4.703746
289.070565	7630.126579	9.015783	-0.058593	4.706121
289.186176	7638.236664	9.020787	-0.058619	4.708545
289.259402	7646.226241	9.025792	-0.058638	4.710931
289.522598	7654.326047	9.030797	-0.058693	4.713349
290.010623	7662.345141	9.035802	-0.058789	4.715740
289.897015	7670.323575	9.040807	-0.058773	4.718120
290.099522	7678.262672	9.045811	-0.058816	4.720487
290.238705	7686.277589	9.050816	-0.058847	4.722874
290.340673	7694.303624	9.055821	-0.058871	4.725264
290.419573	7702.333555	9.060826	-0.058891	4.727654
290.593873	7710.352749	9.065831	-0.058928	4.730039
291.123500	7718.432029	9.070835	-0.059032	4.732440
291.240202	7726.440080	9.075840	-0.059059	4.734820
291.455205	7734.446898	9.080845	-0.059104	4.737197
291.482934	7742.395947	9.085850	-0.059115	4.739557
291.524917	7750.426999	9.090855	-0.059128	4.741940
291.994511	7758.442469	9.095859	-0.059220	4.744316
292.017034	7766.411982	9.100864	-0.059230	4.746679
292.016019	7774.467430	9.105869	-0.059235	4.749065
292.396909	7782.549169	9.110874	-0.059311	4.751457
292.543653	7790.567039	9.115879	-0.059343	4.753830
292.979435	7798.579683	9.120883	-0.059430	4.756199
292.998272	7806.561982	9.125888	-0.059439	4.758559
293.282388	7814.590551	9.130893	-0.059497	4.760931
293.657691	7822.554586	9.135898	-0.059572	4.763282
293.670194	7830.535115	9.140903	-0.059579	4.765639
293.841340	7838.602035	9.145907	-0.059616	4.768018
294.112026	7846.598107	9.150912	-0.059672	4.770376
294.192653	7854.628608	9.155917	-0.059692	4.772743
294.303395	7862.737719	9.160922	-0.059718	4.775132
294.482739	7870.663121	9.165927	-0.059757	4.777465
294.475183	7878.625999	9.170931	-0.059760	4.779809
294.484282	7886.703405	9.175936	-0.059767	4.782186
294.701798	7894.650770	9.180941	-0.059813	4.784522
295.003482	7902.749923	9.185946	-0.059874	4.786901
294.967739	7910.689990	9.190951	-0.059873	4.789234
295.339138	7918.803640	9.195955	-0.059947	4.791615
295.386711	7926.764532	9.200960	-0.059961	4.793951
295.519659	7934.854100	9.205965	-0.059991	4.796323
295.680023	7942.783060	9.210970	-0.060026	4.798647
295.852623	7950.831205	9.215975	-0.060064	4.801005
296.225312	7958.845982	9.220979	-0.060138	4.803351
296.078607	7966.819310	9.225984	-0.060116	4.805686
296.275633	7974.835033	9.230989	-0.060158	4.808031
296.517516	7982.826647	9.235994	-0.060208	4.810367
296.530067	7990.411507	9.240999	-0.060215	4.812584
296.751632	7995.166156	9.246003	-0.060260	4.813972
296.899597	7997.715083	9.251008	-0.060289	4.814716
297.006726	7998.997196	9.256013	-0.060310	4.815090
297.077825	7999.517805	9.261018	-0.060323	4.815242
297.190262	8000.323434	9.266023	-0.060345	4.815477
297.573035	8000.397116	9.271027	-0.060416	4.815497
297.627699	8000.201347	9.276032	-0.060426	4.815439
297.570598	8000.201468	9.281037	-0.060415	4.815439
297.801010	8000.384857	9.286042	-0.060458	4.815492
297.720102	8000.315105	9.291047	-0.060443	4.815472
297.863683	8000.261901	9.296051	-0.060470	4.815456
297.824545	8000.414101	9.301056	-0.060463	4.815500
298.083971	8000.331820	9.306061	-0.060511	4.815475
298.132349	8000.248178	9.311066	-0.060520	4.815450
298.062287	8000.298321	9.316071	-0.060507	4.815465
298.074116	8000.275000	9.321075	-0.060509	4.815459
298.169851	8000.328961	9.326080	-0.060527	4.815474
298.100541	8000.201681	9.331085	-0.060514	4.815437
298.192536	8000.126244	9.336090	-0.060531	4.815414
298.143874	8000.402278	9.341095	-0.060522	4.815495
298.372332	8000.290623	9.346099	-0.060564	4.815462
298.445929	8000.231984	9.351104	-0.060578	4.815444
298.489038	8000.426168	9.356109	-0.060586	4.815501
298.440416	8000.248991	9.361114	-0.060577	4.815449
298.505193	8000.300301	9.366119	-0.060589	4.815464
298.859714	8000.249526	9.371123	-0.060655	4.815447
298.761191	8000.250028	9.376128	-0.060637	4.815448
298.372015	8000.313052	9.381133	-0.060564	4.815468
298.616678	8000.272213	9.386138	-0.060610	4.815455
298.737400	8000.230388	9.391143	-0.060632	4.815442
298.675534	8000.139573	9.396147	-0.060621	4.815416
298.649565	8000.294130	9.401152	-0.060616	4.815461
298.981022	8000.238697	9.406157	-0.060678	4.815444
298.957470	8000.002078	9.411162	-0.060673	4.815375
298.755631	8000.284126	9.416167	-0.060636	4.815458
298.864089	8000.153378	9.421171	-0.060656	4.815419
298.888486	8000.214708	9.426176	-0.060660	4.815437
298.922575	8000.156482	9.431181	-0.060666	4.815420
299.118321	8000.326476	9.436186	-0.060703	4.815468
298.992030	8000.229246	9.441191	-0.060679	4.815441
298.944508	8000.276557	9.446195	-0.060671	4.815455
299.046204	8000.393685	9.451200	-0.060690	4.815488
299.076543	8000.254158	9.456205	-0.060695	4.815448
299.075454	8000.224209	9.461210	-0.060695	4.815439
299.047494	8000.348806	9.466215	-0.060690	4.815475
299.082684	8000.320527	9.471219	-0.060696	4.815467
299.179656	8000.275101	9.476224	-0.060714	4.815453
299.118116	8000.158636	9.481229	-0.060703	4.815419
299.201695	8000.145056	9.486234	-0.060718	4.815415
299.251079	8000.365000	9.491239	-0.060728	4.815479
299.338976	8000.150535	9.496243	-0.060744	4.815416
299.143484	8000.161187	9.501248	-0.060707	4.815420
299.067925	8000.112900	9.506253	-0.060693	4.815406
299.216524	8000.085433	9.511258	-0.060721	4.815398
299.123177	8000.276287	9.516263	-0.060704	4.815454
299.162678	8000.019334	9.521267	-0.060711	4.815379
299.273733	8000.239230	9.526272	-0.060732	4.815442
299.260653	8000.042332	9.531277	-0.060729	4.815385
299.256196	8000.285968	9.536282	-0.060728	4.815456
299.256558	8000.267800	9.541287	-0.060728	4.815451
299.301579	8000.155240	9.546291	-0.060737	4.815418
299.210534	8000.354684	9.551296	-0.060720	4.815476
299.180714	8000.247296	9.556301	-0.060714	4.815445
299.449283	8000.225026	9.561306	-0.060764	4.815437
299.334979	8000.452946	9.566311	-0.060743	4.815504
299.484113	8000.160396	9.571315	-0.060770	4.815418
299.312453	8000.278334	9.576320	-0.060739	4.815454
299.300888	8000.142388	9.581325	-0.060736	4.815414
299.576901	8000.156584	9.586330	-0.060788	4.815417
299.533373	8000.327957	9.591335	-0.060780	4.815467
299.562477	8000.069759	9.596339	-0.060785	4.815391
299.593857	8000.239166	9.601344	-0.060791	4.815441
299.545606	8000.255467	9.606349	-0.060782	4.815446
299.794322	8000.231799	9.611354	-0.060828	4.815438
299.620540	8000.394598	9.616359	-0.060796	4.815486
299.664695	8000.169785	9.621363	-0.060804	4.815420
299.754472	8000.361541	9.626368	-0.060821	4.815476
299.577310	8000.217502	9.631373	-0.060788	4.815434
299.730052	8000.271342	9.636378	-0.060816	4.815449
299.780488	8000.430379	9.641383	-0.060825	4.815496
299.702732	8000.216370	9.646387	-0.060811	4.815434
299.620709	8000.465137	9.651392	-0.060796	4.815507
299.730421	8000.260651	9.656397	-0.060816	4.815446
299.674663	8000.378376	9.661402	-0.060806	4.815481
299.622295	8000.223579	9.666407	-0.060796	4.815436
299.813026	8000.142296	9.671411	-0.060831	4.815411
299.807603	8000.212753	9.676416	-0.060830	4.815432
299.801368	8000.440331	9.681421	-0.060829	4.815498
299.778980	8000.297789	9.686426	-0.060825	4.815457
299.750942	8000.459800	9.691431	-0.060820	4.815504
299.812560	8000.208552	9.696435	-0.060831	4.815431
299.642648	8000.298728	9.701440	-0.060799	4.815458
299.890940	8000.223745	9.706445	-0.060846	4.815435
300.085216	8000.207725	9.711450	-0.060882	4.815429
299.881210	8000.367885	9.716455	-0.060844	4.815477
300.007508	8000.155123	9.721459	-0.060867	4.815414
299.894502	8000.363826	9.726464	-0.060846	4.815476
299.850278	8000.359884	9.731469	-0.060838	4.815475
299.992792	8000.222216	9.736474	-0.060864	4.815434
299.863529	8000.232897	9.741479	-0.060840	4.815438
299.990598	8000.293794	9.746483	-0.060864	4.815455
299.796801	8000.358989	9.751488	-0.060828	4.815475
299.974842	8000.385458	9.756493	-0.060861	4.815482
300.148964	8000.326347	9.761498	-0.060894	4.815464
299.836683	8000.425919	9.766503	-0.060835	4.815494
299.865499	8000.220091	9.771507	-0.060841	4.815434
300.104578	8000.307432	9.776512	-0.060885	4.815458
300.306671	8000.273371	9.781517	-0.060923	4.815447
299.984476	8000.136545	9.786522	-0.060863	4.815409
300.028098	8000.348915	9.791527	-0.060871	4.815471
300.086134	8000.147847	9.796531	-0.060882	4.815412
300.078968	8000.394651	9.801536	-0.060880	4.815484
300.116747	8000.330071	9.806541	-0.060887	4.815465
300.072953	8000.300481	9.811546	-0.060879	4.815456
299.887034	8000.330531	9.816551	-0.060845	4.815466
300.032818	8000.208951	9.821555	-0.060872	4.815430
300.018391	8000.239709	9.826560	-0.060869	4.815439
300.064231	8000.102576	9.831565	-0.060877	4.815399
300.160972	8000.100972	9.836570	-0.060895	4.815398
299.936914	8000.323866	9.841575	-0.060854	4.815464
300.122279	8000.136670	9.846579	-0.060888	4.815408
299.984798	8000.182489	9.851584	-0.060862	4.815422
300.036806	8000.378965	9.856589	-0.060872	4.815479
300.425248	8000.210102	9.861594	-0.060944	4.815428
300.158639	8000.217435	9.866599	-0.060895	4.815432
300.291834	8000.182230	9.871603	-0.060920	4.815421
300.342401	8000.161689	9.876608	-0.060929	4.815414
300.429052	8000.220847	9.881613	-0.060945	4.815431
300.395225	8000.263042	9.886618	-0.060939	4.815444
300.379693	8000.205059	9.891623	-0.060936	4.815427
300.459207	8000.065277	9.896627	-0.060951	4.815386
300.321659	8000.167748	9.901632	-0.060925	4.815416
300.337332	8000.393554	9.906637	-0.060928	4.815482
300.463776	8000.341134	9.911642	-0.060952	4.815466
300.233648	8000.314865	9.916647	-0.060909	4.815460
300.366297	8000.113966	9.921651	-0.060933	4.815400
300.481843	8000.233464	9.926656	-0.060955	4.815435
300.410547	8000.224797	9.931661	-0.060941	4.815433
300.447312	8000.120649	9.936666	-0.060948	4.815402
300.469646	8000.232187	9.941671	-0.060952	4.815434
300.526485	8000.156164	9.946675	-0.060963	4.815412
300.411466	8000.416146	9.951680	-0.060942	4.815488
300.485554	8000.374615	9.956685	-0.060955	4.815476
300.604206	8000.145690	9.961690	-0.060977	4.815409
300.390560	8000.462827	9.966695	-0.060938	4.815502
300.594644	8000.301593	9.971699	-0.060976	4.815454
300.630197	8000.371664	9.976704	-0.060982	4.815474
300.690688	8000.038085	9.981709	-0.060993	4.815377
300.579291	8000.123888	9.986714	-0.060973	4.815402
300.396015	8000.192464	9.991719	-0.060938	4.815423
300.564422	8000.074466	9.996723	-0.060970	4.815388
300.558460	8000.201569	10.001728	-0.060969	4.815425
300.601928	8000.255736	10.006733	-0.060977	4.815441
300.709383	7999.947524	10.011738	-0.060997	4.815350
300.632649	8000.317172	10.016743	-0.060982	4.815459
300.393909	8000.243727	10.021747	-0.060938	4.815438
300.492525	8000.200466	10.026752	-0.060956	4.815425
300.709476	8000.315235	10.031757	-0.060997	4.815458
300.674817	8000.130798	10.036762	-0.060990	4.815404
300.594504	8000.145498	10.041767	-0.060975	4.815409
300.761385	8000.171782	10.046771	-0.061006	4.815415
300.629851	8000.195252	10.051776	-0.060982	4.815423
300.427989	8000.401414	10.056781	-0.060944	4.815484
300.702587	8000.153697	10.061786	-0.060995	4.815410
300.652001	8000.208441	10.066791	-0.060986	4.815427
300.469645	8000.283446	10.071795	-0.060952	4.815449
300.333675	8000.204225	10.076800	-0.060926	4.815427
300.484745	8000.249487	10.081805	-0.060955	4.815439
300.713936	8000.152807	10.086810	-0.060997	4.815410
300.510402	8000.335425	10.091815	-0.060959	4.815464
300.617341	8000.219613	10.096819	-0.060979	4.815430
300.638055	8000.322574	10.101824	-0.060983	4.815460
300.566825	8000.159979	10.106829	-0.060970	4.815413
300.789898	8000.134817	10.111834	-0.061011	4.815404
300.747728	8000.180080	10.116839	-0.061003	4.815418
300.614801	8000.099840	10.121843	-0.060979	4.815395
300.609674	8000.198095	10.126848	-0.060978	4.815424
300.694903	8000.266852	10.131853	-0.060994	4.815444
300.687407	8000.098901	10.136858	-0.060992	4.815395
300.481249	8000.327439	10.141863	-0.060954	4.815462
300.682702	8000.027200	10.146867	-0.060991	4.815374
300.636603	8000.169671	10.151872	-0.060983	4.815415
300.587120	8000.178469	10.156877	-0.060973	4.815418
300.880723	8000.062548	10.161882	-0.061028	4.815383
300.816971	8000.353312	10.166887	-0.061016	4.815468
300.816540	8000.135236	10.171891	-0.061016	4.815404
300.813886	8000.252775	10.176896	-0.061015	4.815439
300.870100	8000.078398	10.181901	-0.061026	4.815388
300.808115	8000.089126	10.186906	-0.061014	4.815391
300.776846	8000.043710	10.191911	-0.061008	4.815378
300.749306	8000.115939	10.196915	-0.061003	4.815399
300.971754	8000.112145	10.201920	-0.061045	4.815397
300.803222	8000.331689	10.206925	-0.061013	4.815462
300.714796	8000.007398	10.211930	-0.060997	4.815368
300.702828	8000.286192	10.216935	-0.060995	4.815449
300.858777	8000.007645	10.221939	-0.061024	4.815367
300.662877	8000.187181	10.226944	-0.060987	4.815420
300.771298	8000.224254	10.231949	-0.061007	4.815431
300.796446	8000.003398	10.236954	-0.061012	4.815366
300.532835	8000.209604	10.241959	-0.060963	4.815428
300.759141	8000.143875	10.246963	-0.061005	4.815407
300.904488	8000.147354	10.251968	-0.061032	4.815408
300.889193	8000.328821	10.256973	-0.061029	4.815461
300.803768	8000.120024	10.261978	-0.061013	4.815400
300.866742	8000.185204	10.266983	-0.061025	4.815419
300.973295	8000.037318	10.271987	-0.061045	4.815375
300.884311	8000.171596	10.276992	-0.061028	4.815415
300.982235	8000.326080	10.281997	-0.061046	4.815459
300.858571	8000.166889	10.287002	-0.061023	4.815414
300.906222	8000.140954	10.292007	-0.061032	4.815406
300.839484	8000.139845	10.297011	-0.061020	4.815406
301.094146	8000.258447	10.302016	-0.061067	4.815439
300.874972	8000.238773	10.307021	-0.061026	4.815434
300.992154	8000.048305	10.312026	-0.061048	4.815378
300.900566	8000.290504	10.317031	-0.061031	4.815449
300.998743	8000.035583	10.322035	-0.061049	4.815375
300.774922	8000.236036	10.327040	-0.061008	4.815434
300.672769	8000.263201	10.332045	-0.060989	4.815443
300.790216	8000.176425	10.337050	-0.061010	4.815417
300.913150	8000.183808	10.342055	-0.061033	4.815418
300.775919	8000.247803	10.347059	-0.061008	4.815438
300.965243	8000.082049	10.352064	-0.061043	4.815388
300.794058	8000.213894	10.357069	-0.061011	4.815428
300.934686	8000.158503	10.362074	-0.061037	4.815411
300.955871	8000.239024	10.367079	-0.061041	4.815434
301.009331	8000.103083	10.372083	-0.061051	4.815394
300.696818	8000.186618	10.377088	-0.060993	4.815420
300.820197	8000.291283	10.382093	-0.061016	4.815450
300.840634	8000.099209	10.387098	-0.061019	4.815394
300.752620	8000.240986	10.392103	-0.061003	4.815436
300.775849	8000.269162	10.397107	-0.061007	4.815444
300.958219	8000.106499	10.402112	-0.061041	4.815395
300.844805	8000.214717	10.407117	-0.061020	4.815428
300.853326	8000.126134	10.412122	-0.061022	4.815402
300.873906	8000.245127	10.417127	-0.061026	4.815436
300.948211	8000.126636	10.422131	-0.061039	4.815401
300.970874	8000.046839	10.427136	-0.061044	4.815378
300.820108	8000.168333	10.432141	-0.061016	4.815414
300.942289	8000.188531	10.437146	-0.061038	4.815419
300.950911	8000.168362	10.442151	-0.061040	4.815414
301.082295	8000.066852	10.447155	-0.061064	4.815383
301.241014	8000.217000	10.452160	-0.061094	4.815426
301.090756	8000.185642	10.457165	-0.061066	4.815418
300.984528	8000.164636	10.462170	-0.061046	4.815412
301.118626	8000.275893	10.467175	-0.061071	4.815444
301.206676	8000.055010	10.472179	-0.061087	4.815379
301.106013	8000.120681	10.477184	-0.061069	4.815399
301.058409	8000.266336	10.482189	-0.061060	4.815442
301.240971	8000.191331	10.487194	-0.061094	4.815419
301.055059	8000.256656	10.492199	-0.061059	4.815439
301.071076	8000.331748	10.497203	-0.061062	4.815461
301.091910	8000.228402	10.502208	-0.061066	4.815430
301.072625	8000.209908	10.507213	-0.061062	4.815425
301.100214	8000.294812	10.512218	-0.061067	4.815450
300.959510	8000.220854	10.517223	-0.061041	4.815429
301.169997	8000.168760	10.522227	-0.061080	4.815413
301.086040	8000.154537	10.527232	-0.061065	4.815409
300.913549	8000.188017	10.532237	-0.061032	4.815419
300.935243	8000.130652	10.537242	-0.061036	4.815403
300.955759	8000.192990	10.542247	-0.061040	4.815421
300.888941	8000.064674	10.547251	-0.061028	4.815384
301.069942	8000.143571	10.552256	-0.061061	4.815406
301.116442	8000.394478	10.557261	-0.061070	4.815479
301.128933	8000.039789	10.562266	-0.061072	4.815375
301.040601	8000.107803	10.567271	-0.061056	4.815395
301.028056	8000.087283	10.572275	-0.061054	4.815390
301.011477	8000.298659	10.577280	-0.061051	4.815451
300.825303	8000.176913	10.582285	-0.061016	4.815417
301.105096	8000.061832	10.587290	-0.061068	4.815382
300.961904	8000.279658	10.592295	-0.061041	4.815446
300.879212	8000.255835	10.597299	-0.061026	4.815439
301.155460	8000.038076	10.602304	-0.061077	4.815375
301.116513	8000.173185	10.607309	-0.061070	4.815414
301.203718	8000.104079	10.612314	-0.061086	4.815394
301.084185	8000.081783	10.617319	-0.061064	4.815388
301.168348	8000.110971	10.622323	-0.061079	4.815396
301.156316	8000.146045	10.627328	-0.061077	4.815406
301.138584	8000.155369	10.632333	-0.061074	4.815409
301.112993	8000.142115	10.637338	-0.061069	4.815405
301.254317	8000.202182	10.642343	-0.061095	4.815422
301.177115	8000.219071	10.647347	-0.061081	4.815427
301.332776	8000.105136	10.652352	-0.061110	4.815393
301.181833	8000.224491	10.657357	-0.061082	4.815429
301.213961	7999.948163	10.662362	-0.061088	4.815348
301.022002	8000.184420	10.667367	-0.061052	4.815418
301.148555	8000.235691	10.672371	-0.061076	4.815432
301.279643	8000.203658	10.677376	-0.061100	4.815422
301.120557	8000.441533	10.682381	-0.061071	4.815493
301.235576	8000.135578	10.687386	-0.061092	4.815403
301.234412	8000.366453	10.692391	-0.061092	4.815470
301.119755	8000.215962	10.697395	-0.061070	4.815427
301.282579	8000.098939	10.702400	-0.061100	4.815392
301.287381	8000.249740	10.707405	-0.061101	4.815436
301.182945	8000.210591	10.712410	-0.061082	4.815425
301.121217	8000.199944	10.717415	-0.061070	4.815422
301.252523	8000.083467	10.722419	-0.061095	4.815387
301.198426	8000.138153	10.727424	-0.061085	4.815404
301.070241	8000.334850	10.732429	-0.061061	4.815462
301.156376	8000.354451	10.737434	-0.061077	4.815467
301.195955	8000.134900	10.742439	-0.061084	4.815403
301.324256	8000.300579	10.747443	-0.061108	4.815450
301.334857	8000.104064	10.752448	-0.061110	4.815393
301.308787	8000.220146	10.757453	-0.061105	4.815427
301.379709	8000.177493	10.762458	-0.061118	4.815414
301.281598	8000.299863	10.767463	-0.061100	4.815450
301.198954	8000.277110	10.772467	-0.061085	4.815444
301.322034	8000.115600	10.777472	-0.061107	4.815396
301.003488	8000.126346	10.782477	-0.061048	4.815401
301.117530	8000.293925	10.787482	-0.061069	4.815449
301.220850	8000.388638	10.792487	-0.061089	4.815477
301.240643	8000.155930	10.797491	-0.061092	4.815409
301.210209	8000.119079	10.802496	-0.061087	4.815398
301.423444	8000.135443	10.807501	-0.061126	4.815402
301.257670	8000.098484	10.812506	-0.061095	4.815392
301.257868	8000.291967	10.817511	-0.061095	4.815448
301.102625	8000.262664	10.822515	-0.061066	4.815440
301.390872	8000.164826	10.827520	-0.061120	4.815410
301.204003	8000.204481	10.832525	-0.061085	4.815423
301.209986	8000.234509	10.837530	-0.061086	4.815432
301.242159	8000.139904	10.842535	-0.061092	4.815404
301.186289	8000.177457	10.847539	-0.061082	4.815415
301.150272	8000.268788	10.852544	-0.061075	4.815442
301.213114	8000.251657	10.857549	-0.061087	4.815437
301.371862	8000.153808	10.862554	-0.061116	4.815407
301.402220	8000.210965	10.867559	-0.061122	4.815424
301.410827	8000.045417	10.872563	-0.061124	4.815375
301.395446	8000.169159	10.877568	-0.061121	4.815412
301.237049	8000.307631	10.882573	-0.061091	4.815453
301.374364	8000.225460	10.887578	-0.061117	4.815428
301.553632	8000.140779	10.892583	-0.061150	4.815403
301.510127	8000.230917	10.897587	-0.061142	4.815429
301.269314	8000.031298	10.902592	-0.061097	4.815372
301.248222	8000.386910	10.907597	-0.061093	4.815476
301.317897	8000.079135	10.912602	-0.061106	4.815386
301.301340	8000.156892	10.917607	-0.061103	4.815409
301.315939	8000.165684	10.922611	-0.061106	4.815411
301.586339	8000.099618	10.927616	-0.061156	4.815390
301.347974	8000.345798	10.932621	-0.061112	4.815464
301.257654	7999.993678	10.937626	-0.061095	4.815361
301.279322	8000.123379	10.942631	-0.061099	4.815399
301.379076	8000.136791	10.947635	-0.061117	4.815402
301.643221	7999.993657	10.952640	-0.061166	4.815359
301.483443	8000.249692	10.957645	-0.061137	4.815435
301.628487	8000.085339	10.962650	-0.061164	4.815386
301.181812	8000.281026	10.967655	-0.061081	4.815445
301.361934	8000.192083	10.972659	-0.061114	4.815419
301.448304	8000.054550	10.977664	-0.061130	4.815378
301.371982	8000.216832	10.982669	-0.061116	4.815426
301.413600	8000.103142	10.987674	-0.061124	4.815392
301.426455	8000.131147	10.992679	-0.061126	4.815400
301.507553	8000.220146	10.997683	-0.061141	4.815426
301.490891	8000.095868	11.002688	-0.061138	4.815390
301.546537	8000.113893	11.007693	-0.061148	4.815395
301.819563	8000.000836	11.012698	-0.061199	4.815360
301.639516	8000.059846	11.017703	-0.061165	4.815379
301.552789	8000.193094	11.022707	-0.061149	4.815418
301.513411	8000.054542	11.027712	-0.061142	4.815378
301.445703	8000.247968	11.032717	-0.061129	4.815434
301.610623	8000.063635	11.037722	-0.061160	4.815380
301.590058	8000.081464	11.042727	-0.061156	4.815385
301.625783	8000.027538	11.047731	-0.061163	4.815369
301.697962	8000.074699	11.052736	-0.061176	4.815383
301.482516	8000.008053	11.057741	-0.061136	4.815364
301.401245	8000.079391	11.062746	-0.061121	4.815385
301.345925	8000.027162	11.067751	-0.061111	4.815370
301.403502	8000.316735	11.072755	-0.061121	4.815455
301.814944	7999.938735	11.077760	-0.061198	4.815342
301.646443	8000.239522	11.082765	-0.061167	4.815431
301.627367	7999.959135	11.087770	-0.061163	4.815349
301.515428	8000.177481	11.092775	-0.061142	4.815414
301.537927	8000.084853	11.097779	-0.061146	4.815386
301.657099	8000.036588	11.102784	-0.061168	4.815372
301.337408	8000.262176	11.107789	-0.061109	4.815439
301.719118	7999.988441	11.112794	-0.061180	4.815357
301.527203	8000.152012	11.117799	-0.061144	4.815406
301.501706	8000.112035	11.122803	-0.061139	4.815395
301.656686	8000.072916	11.127808	-0.061168	4.815382
301.533901	8000.163876	11.132813	-0.061145	4.815409
301.577713	8000.037395	11.137818	-0.061153	4.815372
301.372076	8000.296945	11.142823	-0.061115	4.815449
301.409825	8000.240914	11.147827	-0.061122	4.815433
301.595657	7999.942550	11.152832	-0.061157	4.815345
301.579856	8000.238388	11.157837	-0.061154	4.815431
301.593183	8000.109262	11.162842	-0.061156	4.815393
301.606404	8000.182170	11.167847	-0.061159	4.815414
301.392462	8000.217099	11.172851	-0.061119	4.815426
301.531679	7999.966065	11.177856	-0.061145	4.815352
301.623603	8000.270105	11.182861	-0.061162	4.815440
301.600744	8000.172447	11.187866	-0.061158	4.815412
301.523142	8000.146571	11.192871	-0.061143	4.815404
301.843854	8000.286584	11.197875	-0.061203	4.815444
301.653032	7999.988379	11.202880	-0.061167	4.815358
301.538646	8000.307168	11.207885	-0.061146	4.815451
301.689007	8000.083041	11.212890	-0.061174	4.815385
301.590672	8000.247096	11.217895	-0.061156	4.815434
301.654116	8000.147665	11.222899	-0.061167	4.815404
301.655339	8000.003373	11.227904	-0.061167	4.815362
301.571906	8000.310918	11.232909	-0.061152	4.815452
301.746160	8000.229360	11.237914	-0.061185	4.815428
301.636092	8000.287393	11.242919	-0.061164	4.815445
301.600486	8000.118972	11.247923	-0.061157	4.815396
301.701268	8000.025505	11.252928	-0.061176	4.815368
301.578394	8000.149601	11.257933	-0.061153	4.815405
301.674618	8000.130886	11.262938	-0.061171	4.815399
302.011991	8000.054174	11.267943	-0.061234	4.815375
301.894094	8000.185836	11.272947	-0.061212	4.815414
301.680429	7999.947116	11.277952	-0.061172	4.815345
301.746800	8000.164146	11.282957	-0.061184	4.815409
301.781353	7999.965890	11.287962	-0.061191	4.815350
301.857088	8000.179869	11.292967	-0.061205	4.815413
301.872708	8000.046505	11.297971	-0.061208	4.815374
301.798249	8000.088026	11.302976	-0.061194	4.815386
301.572511	8000.177277	11.307981	-0.061152	4.815413
301.779391	8000.048158	11.312986	-0.061190	4.815375
301.789390	8000.158425	11.317991	-0.061192	4.815407
301.760371	8000.054252	11.322995	-0.061187	4.815376
301.663970	7999.972478	11.328000	-0.061169	4.815353
301.852729	8000.072885	11.333005	-0.061204	4.815381
301.843740	7999.987216	11.338010	-0.061202	4.815356
301.682011	8000.081806	11.343015	-0.061172	4.815385
301.763143	8000.146219	11.348019	-0.061187	4.815403
301.934671	7999.982306	11.353024	-0.061219	4.815355
301.828746	8000.069270	11.358029	-0.061199	4.815380
301.754010	7999.920511	11.363034	-0.061185	4.815337
301.720474	8000.058917	11.368039	-0.061179	4.815378
301.659574	8000.283457	11.373043	-0.061168	4.815444
301.896471	7999.998766	11.378048	-0.061212	4.815360
301.725215	8000.188335	11.383053	-0.061180	4.815416
301.955447	7999.854362	11.388058	-0.061223	4.815317
301.894457	8000.059658	11.393063	-0.061211	4.815377
301.913820	8000.159391	11.398067	-0.061215	4.815406
301.939571	8000.140575	11.403072	-0.061220	4.815401
301.754715	8000.151401	11.408077	-0.061185	4.815405
301.536360	7999.950018	11.413082	-0.061145	4.815347
301.882464	8000.148173	11.418087	-0.061209	4.815403
301.743860	8000.088146	11.423091	-0.061183	4.815386
301.734953	8000.106169	11.428096	-0.061182	4.815392
301.563154	8000.241212	11.433101	-0.061150	4.815432
301.784367	8000.133710	11.438106	-0.061191	4.815399
301.751831	8000.286031	11.443111	-0.061185	4.815444
301.683397	8000.133099	11.448115	-0.061172	4.815400
302.134535	8000.195104	11.453120	-0.061256	4.815416
301.737159	8000.130780	11.458125	-0.061182	4.815399
301.680342	8000.004767	11.463130	-0.061171	4.815362
301.882401	8000.182360	11.468135	-0.061209	4.815413
301.846197	8000.214896	11.473139	-0.061202	4.815423
301.784948	8000.000083	11.478144	-0.061191	4.815360
301.638527	8000.137685	11.483149	-0.061163	4.815401
301.724901	8000.036496	11.488154	-0.061179	4.815371
301.804296	8000.230227	11.493159	-0.061194	4.815428
301.713875	8000.221241	11.498163	-0.061177	4.815425
301.869630	7999.983307	11.503168	-0.061206	4.815355
301.749985	8000.135250	11.508173	-0.061184	4.815400
301.692991	8000.066957	11.513178	-0.061173	4.815380
301.867234	8000.085882	11.518183	-0.061206	4.815385
301.815794	8000.182302	11.523187	-0.061196	4.815414
301.758232	7999.917311	11.528192	-0.061185	4.815336
301.792269	8000.143425	11.533197	-0.061192	4.815402
302.013766	8000.066927	11.538202	-0.061233	4.815379
301.973355	8000.028841	11.543207	-0.061225	4.815368
301.750974	8000.087147	11.548211	-0.061184	4.815386
301.994211	7999.989631	11.553216	-0.061229	4.815356
301.835641	7999.990204	11.558221	-0.061200	4.815357
301.718234	8000.026736	11.563226	-0.061178	4.815369
301.885160	7999.987815	11.568231	-0.061209	4.815356
301.962452	8000.108821	11.573235	-0.061223	4.815391
301.889208	7999.892741	11.578240	-0.061209	4.815329
301.686673	8000.089274	11.583245	-0.061172	4.815387
302.145555	8000.042371	11.588250	-0.061257	4.815371
302.063308	7999.996107	11.593255	-0.061242	4.815358
301.973565	8000.085478	11.598259	-0.061225	4.815385
301.983983	8000.053580	11.603264	-0.061227	4.815375
301.920179	8000.157278	11.608269	-0.061215	4.815406
302.089982	7999.984784	11.613274	-0.061247	4.815355
302.015160	8000.137472	11.618279	-0.061233	4.815399
301.992316	8000.102883	11.623283	-0.061229	4.815390
302.093641	8000.011563	11.628288	-0.061247	4.815362
301.752297	8000.128826	11.633293	-0.061184	4.815398
302.072227	8000.222861	11.638298	-0.061243	4.815424
302.026655	8000.057480	11.643303	-0.061235	4.815376
301.975036	8000.205209	11.648307	-0.061225	4.815419
301.947050	8000.112810	11.653312	-0.061220	4.815393
301.964029	8000.182573	11.658317	-0.061223	4.815413
301.993058	8000.087915	11.663322	-0.061229	4.815385
301.926241	8000.139183	11.668327	-0.061216	4.815400
301.962295	8000.253092	11.673331	-0.061223	4.815434
301.931854	8000.091169	11.678336	-0.061217	4.815386
301.846130	8000.012779	11.683341	-0.061201	4.815364
301.948204	8000.141678	11.688346	-0.061220	4.815401
302.130193	8000.140422	11.693351	-0.061254	4.815400
302.112364	8000.177538	11.698355	-0.061251	4.815411
302.042354	7999.868511	11.703360	-0.061237	4.815321
302.033522	8000.171949	11.708365	-0.061236	4.815409
301.918551	8000.111245	11.713370	-0.061214	4.815392
301.883163	8000.150208	11.718375	-0.061208	4.815404
302.155097	8000.042478	11.723379	-0.061258	4.815371
302.236213	7999.954029	11.728384	-0.061273	4.815345
302.065664	8000.240888	11.733389	-0.061242	4.815429
302.092122	8000.132289	11.738394	-0.061247	4.815398
302.145028	8000.117131	11.743399	-0.061257	4.815393
302.110512	8000.273696	11.748403	-0.061250	4.815439
302.094681	8000.039326	11.753408	-0.061247	4.815370
301.948315	8000.123481	11.758413	-0.061220	4.815396
302.149918	8000.034894	11.763418	-0.061257	4.815369
302.065972	8000.099775	11.768423	-0.061242	4.815388
302.106180	8000.142130	11.773427	-0.061249	4.815400
302.034816	8000.100322	11.778432	-0.061236	4.815389
301.837176	8000.238144	11.783437	-0.061199	4.815430
302.119581	8000.005518	11.788442	-0.061252	4.815360
301.994053	8000.011985	11.793447	-0.061228	4.815363
302.136664	7999.981212	11.798451	-0.061255	4.815353
302.277674	8000.011344	11.803456	-0.061281	4.815361
302.280398	8000.096905	11.808461	-0.061281	4.815386
302.190643	7999.935067	11.813466	-0.061265	4.815340
302.148971	8000.032719	11.818471	-0.061257	4.815368
302.157167	8000.044612	11.823475	-0.061258	4.815372
302.207098	7999.921438	11.828480	-0.061268	4.815335
301.959216	8000.004977	11.833485	-0.061221	4.815361
301.925455	8000.065346	11.838490	-0.061215	4.815379
302.255508	8000.088996	11.843495	-0.061277	4.815384
302.114457	8000.189274	11.848499	-0.061250	4.815414
301.975179	8000.044786	11.853504	-0.061224	4.815373
302.187519	8000.189414	11.858509	-0.061264	4.815414
302.281794	8000.136459	11.863514	-0.061281	4.815398
302.177309	8000.133654	11.868519	-0.061262	4.815398
302.238022	7999.968969	11.873523	-0.061273	4.815349
302.200504	8000.039965	11.878528	-0.061266	4.815370
302.151332	8000.064802	11.883533	-0.061257	4.815378
302.097834	7999.955947	11.888538	-0.061247	4.815346
302.134483	8000.004656	11.893543	-0.061254	4.815360
302.052311	8000.071705	11.898547	-0.061239	4.815380
302.093529	8000.027490	11.903552	-0.061246	4.815367
302.068650	7999.998213	11.908557	-0.061242	4.815359
302.150047	8000.113942	11.913562	-0.061257	4.815392
302.206500	8000.005842	11.918567	-0.061267	4.815360
302.124534	8000.111377	11.923571	-0.061252	4.815391
302.339246	8000.117078	11.928576	-0.061292	4.815392
302.082862	8000.204751	11.933581	-0.061244	4.815419
302.056908	8000.010834	11.938586	-0.061239	4.815362
302.305863	8000.090862	11.943591	-0.061286	4.815385
302.105648	8000.178399	11.948595	-0.061248	4.815411
302.059242	8000.034385	11.953600	-0.061240	4.815369
302.102579	8000.290588	11.958605	-0.061248	4.815444
302.196516	8000.131798	11.963610	-0.061265	4.815397
302.301277	8000.046948	11.968615	-0.061285	4.815372
302.392344	8000.139322	11.973619	-0.061302	4.815398
302.385042	7999.908300	11.978624	-0.061300	4.815331
302.298076	8000.117442	11.983629	-0.061284	4.815392
302.154259	7999.952569	11.988634	-0.061257	4.815345
302.232887	8000.103528	11.993639	-0.061272	4.815389
302.222587	8000.167494	11.998643	-0.061270	4.815407
302.223874	8000.049926	12.003648	-0.061270	4.815373
302.420051	8000.171838	12.008653	-0.061307	4.815408
302.555870	8000.008399	12.013658	-0.061332	4.815359
302.335595	7999.988705	12.018663	-0.061291	4.815355
302.194731	8000.102883	12.023667	-0.061265	4.815389
302.307796	7999.995723	12.028672	-0.061286	4.815357
302.358524	8000.019011	12.033677	-0.061295	4.815363
302.069329	7999.989623	12.038682	-0.061241	4.815356
302.393380	8000.133967	12.043687	-0.061301	4.815397
302.312937	8000.156147	12.048691	-0.061287	4.815404
302.309220	8000.113324	12.053696	-0.061286	4.815391
302.225124	8000.123685	12.058701	-0.061270	4.815395
302.193347	7999.991672	12.063706	-0.061264	4.815356
302.264385	7999.983228	12.068711	-0.061277	4.815353
302.049253	8000.171001	12.073715	-0.061237	4.815409
302.303320	7999.950732	12.078720	-0.061284	4.815344
302.271652	8000.124448	12.083725	-0.061279	4.815395
302.276408	8000.033662	12.088730	-0.061279	4.815368
302.271378	8000.096646	12.093735	-0.061279	4.815386
302.144836	8000.108440	12.098739	-0.061255	4.815390
302.202644	7999.845362	12.103744	-0.061266	4.815313
302.225334	8000.132221	12.108749	-0.061270	4.815397
302.257545	8000.004477	12.113754	-0.061276	4.815360
302.062296	7999.945648	12.118759	-0.061239	4.815343
302.034954	8000.080951	12.123763	-0.061234	4.815383
302.153999	7999.971752	12.128768	-0.061256	4.815350
302.269553	8000.163946	12.133773	-0.061278	4.815406
302.321684	7999.965980	12.138778	-0.061288	4.815348
302.439020	8000.173170	12.143783	-0.061310	4.815408
302.247543	8000.114402	12.148787	-0.061274	4.815392
302.295209	7999.919569	12.153792	-0.061283	4.815335
302.321795	8000.051492	12.158797	-0.061288	4.815373
302.468534	8000.143721	12.163802	-0.061315	4.815399
302.504053	8000.200965	12.168807	-0.061322	4.815416
302.202240	8000.169227	12.173811	-0.061265	4.815408
302.293004	8000.071317	12.178816	-0.061282	4.815379
302.552939	8000.150459	12.183821	-0.061331	4.815401
302.342185	7999.948128	12.188826	-0.061291	4.815343
302.444813	7999.941278	12.193831	-0.061310	4.815340
302.465373	8000.035688	12.198835	-0.061314	4.815368
302.547081	8000.002835	12.203840	-0.061329	4.815358
302.557440	8000.092799	12.208845	-0.061331	4.815384
302.423596	8000.117300	12.213850	-0.061306	4.815392
302.347434	7999.986687	12.218855	-0.061292	4.815354
302.396500	8000.020638	12.223859	-0.061301	4.815364
302.458242	8000.190560	12.228864	-0.061313	4.815413
302.311993	8000.054507	12.233869	-0.061285	4.815374
302.247634	8000.136817	12.238874	-0.061274	4.815398
302.324495	7999.849469	12.243879	-0.061288	4.815314
302.249220	8000.131495	12.248883	-0.061274	4.815397
302.345579	7999.962056	12.253888	-0.061292	4.815347
302.273235	8000.050647	12.258893	-0.061278	4.815373
302.425576	8000.159004	12.263898	-0.061307	4.815404
302.624593	7999.955993	12.268903	-0.061343	4.815344
302.433569	8000.127063	12.273907	-0.061308	4.815395
302.600446	7999.922450	12.278912	-0.061339	4.815334
302.507822	8000.273675	12.283917	-0.061322	4.815437
302.324500	8000.070728	12.288922	-0.061288	4.815379
302.440009	8000.058747	12.293927	-0.061309	4.815375
302.378917	8000.143250	12.298931	-0.061298	4.815399
302.447998	7999.968013	12.303936	-0.061310	4.815348
302.469262	8000.093435	12.308941	-0.061314	4.815385
302.379160	8000.195628	12.313946	-0.061298	4.815415
302.322350	8000.097406	12.318951	-0.061287	4.815386
302.276527	8000.070988	12.323955	-0.061278	4.815379
302.406268	8000.034656	12.328960	-0.061303	4.815368
302.491954	8000.002939	12.333965	-0.061319	4.815358
302.409168	7999.990873	12.338970	-0.061303	4.815355
302.361078	8000.073453	12.343975	-0.061294	4.815379
302.502488	8000.026625	12.348979	-0.061320	4.815365
302.607739	7999.966370	12.353984	-0.061340	4.815347
302.408010	8000.049639	12.358989	-0.061303	4.815372
302.449180	8000.139047	12.363994	-0.061311	4.815398
302.669398	8000.046492	12.368999	-0.061351	4.815370
302.426066	7999.960139	12.374003	-0.061306	4.815346
302.570452	7999.916568	12.379008	-0.061333	4.815332
302.625480	8000.253142	12.384013	-0.061343	4.815430
302.437214	7999.988112	12.389018	-0.061308	4.815354
302.395999	8000.112496	12.394023	-0.061300	4.815390
302.430795	8000.211419	12.399027	-0.061307	4.815419
302.373922	8000.026608	12.404032	-0.061296	4.815365
302.252237	8000.214864	12.409037	-0.061274	4.815421
302.182666	8000.259673	12.414042	-0.061261	4.815434
302.579360	8000.008633	12.419047	-0.061334	4.815359
302.312451	8000.176306	12.424051	-0.061285	4.815409
302.478685	8000.020854	12.429056	-0.061316	4.815363
302.541950	8000.174768	12.434061	-0.061327	4.815408
302.564550	8000.143071	12.439066	-0.061332	4.815399
302.402855	8000.048452	12.444071	-0.061301	4.815372
302.582004	8000.214980	12.449075	-0.061335	4.815419
302.707317	7999.946605	12.454080	-0.061358	4.815340
302.634760	8000.058711	12.459085	-0.061345	4.815374
302.454132	7999.954157	12.464090	-0.061311	4.815344
302.708454	8000.050309	12.469095	-0.061358	4.815371
302.431558	8000.204989	12.474099	-0.061307	4.815417
302.416939	8000.185502	12.479104	-0.061304	4.815412
302.624410	8000.067081	12.484109	-0.061343	4.815376
302.420505	8000.063694	12.489114	-0.061305	4.815376
302.539618	8000.092394	12.494119	-0.061327	4.815384
302.576289	8000.127208	12.499123	-0.061334	4.815394
302.746995	8000.176008	12.504128	-0.061365	4.815407
302.837991	8000.213863	12.509133	-0.061382	4.815418
302.877926	8000.102280	12.514138	-0.061390	4.815385
302.807467	8000.146006	12.519143	-0.061377	4.815398
302.537726	8000.209940	12.524147	-0.061326	4.815418
302.566520	8000.092827	12.529152	-0.061332	4.815384
302.482229	8000.113874	12.534157	-0.061316	4.815390
302.497846	8000.213548	12.539162	-0.061319	4.815419
302.475900	8000.064592	12.544167	-0.061315	4.815376
302.636752	8000.226541	12.549171	-0.061345	4.815423
302.708306	8000.115483	12.554176	-0.061358	4.815390
302.671328	8000.204662	12.559181	-0.061351	4.815416
302.575795	8000.174211	12.564186	-0.061333	4.815408
302.772016	8000.111190	12.569191	-0.061370	4.815388
302.601830	8000.114776	12.574195	-0.061338	4.815390
302.567426	8000.022270	12.579200	-0.061332	4.815363
302.644564	8000.074860	12.584205	-0.061346	4.815378
302.600070	7999.930876	12.589210	-0.061337	4.815336
302.591911	8000.109259	12.594215	-0.061336	4.815389
302.462095	8000.255691	12.599219	-0.061312	4.815432
302.609447	7999.925681	12.604224	-0.061339	4.815335
302.614155	8000.230418	12.609229	-0.061340	4.815424
302.562929	8000.056389	12.614234	-0.061331	4.815373
302.728271	8000.058064	12.619239	-0.061361	4.815373
302.607440	8000.062470	12.624243	-0.061339	4.815375
302.640863	8000.127162	12.629248	-0.061345	4.815394
302.784609	8000.184066	12.634253	-0.061372	4.815409
302.737563	8000.088142	12.639258	-0.061363	4.815382
302.750739	8000.218776	12.644263	-0.061365	4.815420
302.545854	8000.278442	12.649267	-0.061327	4.815438
302.747468	8000.074404	12.654272	-0.061365	4.815378
302.814554	8000.207002	12.659277	-0.061377	4.815416
302.703442	8000.256467	12.664282	-0.061357	4.815431
302.726940	8000.087954	12.669287	-0.061361	4.815382
302.729956	8000.090140	12.674291	-0.061361	4.815382
302.781473	8000.089925	12.679296	-0.061371	4.815382
302.730194	8000.117934	12.684301	-0.061361	4.815390
302.872944	8000.085026	12.689306	-0.061388	4.815380
302.905593	8000.139016	12.694311	-0.061394	4.815396
302.719262	8000.226784	12.699315	-0.061359	4.815422
302.886831	8000.168632	12.704320	-0.061391	4.815404
302.863950	8000.069903	12.709325	-0.061386	4.815376
302.848056	8000.167985	12.714330	-0.061383	4.815404
302.993362	8000.220639	12.719335	-0.061410	4.815419
302.919172	8000.192680	12.724339	-0.061396	4.815411
302.658704	8000.174455	12.729344	-0.061348	4.815407
302.827277	8000.226427	12.734349	-0.061379	4.815422
302.944365	8000.257233	12.739354	-0.061401	4.815430
302.821048	8000.073453	12.744359	-0.061378	4.815377
302.884213	8000.405891	12.749363	-0.061390	4.815474
302.964947	8000.254362	12.754368	-0.061405	4.815429
302.901565	8000.169925	12.759373	-0.061393	4.815405
302.890117	8000.240287	12.764378	-0.061391	4.815425
302.898005	8000.055480	12.769383	-0.061392	4.815371
302.926627	8000.219509	12.774387	-0.061398	4.815419
302.934826	8000.073191	12.779392	-0.061399	4.815376
303.133409	8000.226147	12.784397	-0.061436	4.815420
303.036429	8000.504616	12.789402	-0.061418	4.815502
302.988084	8000.173486	12.794407	-0.061409	4.815405
302.806225	8000.360747	12.799411	-0.061375	4.815461
302.937407	8000.122398	12.804416	-0.061400	4.815391
303.031999	8000.053413	12.809421	-0.061417	4.815370
302.798484	7999.954394	12.814426	-0.061373	4.815342
302.916920	8000.011946	12.819431	-0.061396	4.815359
303.027055	8000.188019	12.824435	-0.061416	4.815409
303.082790	8000.090595	12.829440	-0.061426	4.815381
302.965215	8000.100399	12.834445	-0.061405	4.815384
302.983983	8000.287784	12.839450	-0.061408	4.815439
302.953863	8000.093793	12.844455	-0.061402	4.815382
302.891649	8000.184692	12.849459	-0.061391	4.815409
303.050581	8000.139224	12.854464	-0.061420	4.815395
303.163025	8000.142159	12.859469	-0.061441	4.815395
303.020331	8000.075647	12.864474	-0.061415	4.815377
303.155996	8000.098209	12.869479	-0.061440	4.815383
303.217768	8000.132372	12.874483	-0.061451	4.815392
303.077323	8000.014586	12.879488	-0.061425	4.815359
303.167874	8000.179645	12.884493	-0.061442	4.815406
302.993365	8000.085880	12.889498	-0.061410	4.815380
303.010250	7999.980328	12.894503	-0.061413	4.815349
302.839997	8000.227644	12.899507	-0.061381	4.815422
302.910241	7999.936973	12.904512	-0.061394	4.815337
302.876672	8000.219697	12.909517	-0.061388	4.815419
302.687018	8000.261443	12.914522	-0.061352	4.815433
302.900001	8000.050110	12.919527	-0.061392	4.815370
302.873475	8000.259191	12.924531	-0.061387	4.815431
302.947589	8000.000654	12.929536	-0.061401	4.815355
302.895570	8000.255278	12.934541	-0.061391	4.815430
302.825848	8000.208151	12.939546	-0.061378	4.815416
303.042881	8000.239548	12.944551	-0.061419	4.815424
303.014667	8000.234802	12.949555	-0.061413	4.815423
303.065608	8000.144780	12.954560	-0.061423	4.815397
303.013689	8000.116122	12.959565	-0.061413	4.815389
302.939657	8000.110615	12.964570	-0.061399	4.815387
302.807984	8000.091323	12.969575	-0.061375	4.815382
303.021214	8000.146174	12.974579	-0.061414	4.815397
303.254594	8000.073080	12.979584	-0.061458	4.815375
302.953854	8000.183535	12.984589	-0.061402	4.815409
302.925853	8000.230104	12.989594	-0.061397	4.815422
302.909955	7999.947624	12.994599	-0.061393	4.815340
302.908682	8000.052362	12.999603	-0.061393	4.815370
302.869117	8000.019633	13.004608	-0.061386	4.815361
302.960603	8000.007253	13.009613	-0.061403	4.815357
303.007877	7999.999484	13.014618	-0.061412	4.815355
303.044144	8000.030016	13.019623	-0.061418	4.815363
302.853226	8000.141226	13.024627	-0.061383	4.815397
302.998984	7999.907398	13.029632	-0.061410	4.815328
302.897183	8000.066054	13.034637	-0.061391	4.815375
302.877243	8000.069997	13.039642	-0.061387	4.815376
303.072937	7999.918241	13.044647	-0.061424	4.815331
302.840586	8000.250045	13.049651	-0.061381	4.815429
302.744847	8000.083828	13.054656	-0.061363	4.815380
303.020280	8000.061675	13.059661	-0.061414	4.815373
302.951802	8000.168504	13.064666	-0.061401	4.815404
302.996788	7999.953313	13.069671	-0.061409	4.815341
303.065821	8000.083805	13.074675	-0.061422	4.815379
302.949813	8000.087222	13.079680	-0.061401	4.815380
302.976953	7999.926253	13.084685	-0.061406	4.815333
303.047254	8000.143355	13.089690	-0.061419	4.815396
303.008134	8000.080701	13.094695	-0.061411	4.815378
303.146872	8000.078727	13.099699	-0.061437	4.815377
303.143859	8000.022019	13.104704	-0.061437	4.815360
303.261568	8000.257015	13.109709	-0.061459	4.815429
303.014015	8000.014514	13.114714	-0.061412	4.815359
302.998589	8000.016394	13.119719	-0.061409	4.815360
303.024610	8000.175035	13.124723	-0.061414	4.815406
303.275156	8000.122538	13.129728	-0.061461	4.815389
303.026312	8000.084195	13.134733	-0.061415	4.815379
302.984363	8000.133739	13.139738	-0.061407	4.815394
303.309760	8000.027965	13.144743	-0.061467	4.815361
303.059753	8000.075123	13.149747	-0.061421	4.815376
302.951051	8000.004901	13.154752	-0.061400	4.815356
303.077858	7999.998453	13.159757	-0.061424	4.815354
303.031991	8000.059691	13.164762	-0.061416	4.815372
303.281882	8000.029631	13.169767	-0.061462	4.815362
303.184107	8000.093214	13.174771	-0.061444	4.815381
303.238667	7999.927355	13.179776	-0.061454	4.815332
303.304994	8000.209602	13.184781	-0.061466	4.815414
303.152461	8000.102304	13.189786	-0.061438	4.815384
303.373733	7999.850486	13.194791	-0.061479	4.815309
303.196287	8000.034612	13.199795	-0.061446	4.815364
303.149286	8000.053071	13.204800	-0.061437	4.815370
303.073715	8000.105264	13.209805	-0.061423	4.815385
303.077888	8000.016605	13.214810	-0.061424	4.815359
303.164756	7999.976355	13.219815	-0.061440	4.815347
303.181069	8000.034349	13.224819	-0.061443	4.815364
303.296574	7999.978540	13.229824	-0.061464	4.815347
303.204398	7999.947076	13.234829	-0.061447	4.815338
302.948553	8000.082863	13.239834	-0.061400	4.815379
303.169915	7999.962534	13.244839	-0.061441	4.815343
303.135717	8000.147970	13.249843	-0.061435	4.815397
303.075614	8000.099933	13.254848	-0.061423	4.815384
303.176778	8000.017161	13.259853	-0.061442	4.815359
303.178312	8000.001149	13.264858	-0.061442	4.815354
303.215814	8000.000701	13.269863	-0.061449	4.815354
302.902710	8000.073537	13.274867	-0.061391	4.815377
303.016953	7999.899049	13.279872	-0.061412	4.815325
303.272843	7999.951400	13.284877	-0.061460	4.815339
303.006788	7999.927739	13.289882	-0.061410	4.815334
303.306517	7999.925230	13.294887	-0.061466	4.815331
303.320809	7999.916914	13.299891	-0.061469	4.815329
303.359587	7999.858761	13.304896	-0.061476	4.815312
303.572036	7999.912530	13.309901	-0.061515	4.815326
303.233936	8000.090781	13.314906	-0.061452	4.815380
303.324834	7999.902007	13.319911	-0.061469	4.815325
303.233100	8000.155972	13.324915	-0.061452	4.815399
303.327027	8000.022836	13.329920	-0.061470	4.815360
303.343388	8000.096867	13.334925	-0.061473	4.815381
303.392118	8000.069880	13.339930	-0.061482	4.815373
303.383311	7999.834553	13.344935	-0.061480	4.815305
303.205701	8000.058228	13.349939	-0.061447	4.815371
303.040312	8000.075791	13.354944	-0.061416	4.815377
303.229924	7999.977383	13.359949	-0.061451	4.815347
303.304226	8000.189209	13.364954	-0.061465	4.815409
303.135275	7999.937324	13.369959	-0.061434	4.815336
303.096387	8000.055334	13.374963	-0.061427	4.815370
303.511797	7999.973504	13.379968	-0.061504	4.815345
303.328861	7999.982223	13.384973	-0.061470	4.815348
303.081727	7999.971704	13.389978	-0.061424	4.815346
303.168805	7999.923974	13.394983	-0.061440	4.815332
303.343388	7999.957872	13.399987	-0.061472	4.815341
303.375729	7999.904957	13.404992	-0.061478	4.815325
303.488644	7999.907899	13.409997	-0.061499	4.815326
303.384359	8000.200142	13.415002	-0.061480	4.815411
303.466773	7999.942809	13.420007	-0.061495	4.815336
303.365694	8000.029856	13.425011	-0.061477	4.815362
303.399162	7999.984443	13.430016	-0.061483	4.815348
303.355032	7999.991191	13.435021	-0.061474	4.815350
303.245750	8000.221348	13.440026	-0.061454	4.815418
303.473077	7999.826384	13.445031	-0.061496	4.815302
303.435814	8000.168912	13.450035	-0.061490	4.815402
303.234061	7999.999864	13.455040	-0.061452	4.815354
303.224244	7999.933422	13.460045	-0.061450	4.815334
303.374198	8000.155055	13.465050	-0.061478	4.815398
303.494430	8000.006320	13.470055	-0.061500	4.815354
303.254807	8000.005546	13.475059	-0.061456	4.815355
303.290921	8000.020041	13.480064	-0.061462	4.815359
303.499781	8000.006403	13.485069	-0.061501	4.815354
303.306946	7999.998923	13.490074	-0.061465	4.815353
303.246023	8000.050290	13.495079	-0.061454	4.815368
303.351794	8000.088391	13.500083	-0.061474	4.815379
303.398704	7999.997234	13.505088	-0.061482	4.815352
303.416701	7999.918425	13.510093	-0.061486	4.815329
303.425795	8000.092821	13.515098	-0.061487	4.815380
303.314993	7999.956285	13.520103	-0.061467	4.815340
303.216310	8000.257172	13.525107	-0.061448	4.815429
303.128228	8000.126358	13.530112	-0.061432	4.815391
303.290977	7999.918466	13.535117	-0.061462	4.815330
303.256476	8000.108173	13.540122	-0.061456	4.815385
303.234639	8000.145223	13.545127	-0.061452	4.815396
303.285995	7999.996414	13.550131	-0.061461	4.815352
303.360791	8000.089588	13.555136	-0.061475	4.815379
303.322932	7999.853779	13.560141	-0.061468	4.815311
303.121987	8000.007582	13.565146	-0.061431	4.815356
303.410009	7999.861635	13.570151	-0.061484	4.815312
303.318938	8000.068575	13.575155	-0.061467	4.815373
303.374392	7999.931593	13.580160	-0.061477	4.815333
303.382936	8000.038633	13.585165	-0.061479	4.815364
303.360642	8000.138747	13.590170	-0.061475	4.815394
303.416130	7999.902348	13.595175	-0.061485	4.815324
303.546916	7999.979348	13.600179	-0.061509	4.815346
303.519229	8000.048372	13.605184	-0.061504	4.815366
303.535205	7999.985564	13.610189	-0.061507	4.815348
303.442902	8000.162553	13.615194	-0.061490	4.815400
303.324938	8000.216180	13.620199	-0.061468	4.815416
303.381347	8000.218184	13.625203	-0.061479	4.815417
303.411922	8000.116065	13.630208	-0.061484	4.815387
303.579274	8000.089980	13.635213	-0.061515	4.815378
303.523867	8000.002468	13.640218	-0.061505	4.815353
303.418691	7999.950476	13.645223	-0.061485	4.815338
303.534858	7999.974853	13.650227	-0.061507	4.815345
303.586264	8000.021672	13.655232	-0.061517	4.815358
303.320298	7999.972355	13.660237	-0.061467	4.815345
303.313517	8000.139004	13.665242	-0.061466	4.815394
303.430560	7999.898283	13.670247	-0.061487	4.815323
303.518431	7999.945707	13.675251	-0.061504	4.815336
303.326577	7999.957485	13.680256	-0.061468	4.815341
303.545870	7999.867053	13.685261	-0.061509	4.815313
303.523677	8000.102932	13.690266	-0.061505	4.815382
303.365687	7999.930335	13.695271	-0.061475	4.815333
303.479501	7999.998501	13.700275	-0.061497	4.815352
303.620305	8000.050012	13.705280	-0.061523	4.815366
303.590354	7999.897714	13.710285	-0.061517	4.815322
303.632272	8000.132521	13.715290	-0.061525	4.815390
303.572936	8000.052426	13.720295	-0.061514	4.815367
303.664494	8000.027220	13.725299	-0.061531	4.815360
303.499315	8000.082201	13.730304	-0.061500	4.815376
303.532188	7999.967293	13.735309	-0.061506	4.815343
303.384659	8000.114501	13.740314	-0.061479	4.815386
303.472952	7999.906441	13.745319	-0.061495	4.815325
303.602750	8000.101015	13.750323	-0.061519	4.815381
303.752943	8000.014781	13.755328	-0.061547	4.815355
303.419263	8000.240142	13.760333	-0.061485	4.815423
303.442215	8000.033134	13.765338	-0.061489	4.815362
303.591750	8000.015304	13.770343	-0.061517	4.815356
303.502355	7999.975334	13.775347	-0.061500	4.815345
303.417432	8000.027372	13.780352	-0.061485	4.815361
303.544048	8000.008092	13.785357	-0.061508	4.815355
303.575997	7999.962654	13.790362	-0.061514	4.815341
303.451756	8000.057868	13.795367	-0.061491	4.815370
303.490519	8000.003991	13.800371	-0.061498	4.815354
303.628636	8000.127081	13.805376	-0.061524	4.815389
303.763650	7999.968970	13.810381	-0.061549	4.815342
303.507427	8000.107959	13.815386	-0.061501	4.815384
303.765761	8000.053453	13.820391	-0.061549	4.815367
303.739320	8000.020941	13.825395	-0.061544	4.815357
303.580780	7999.975546	13.830400	-0.061515	4.815345
303.845779	7999.873045	13.835405	-0.061564	4.815314
303.636190	8000.161401	13.840410	-0.061525	4.815399
303.750673	7999.933464	13.845415	-0.061546	4.815332
303.578687	8000.084542	13.850419	-0.061514	4.815377
303.667696	7999.986601	13.855424	-0.061531	4.815348
303.661483	7999.893493	13.860429	-0.061530	4.815321
303.705696	8000.041748	13.865434	-0.061538	4.815364
303.812866	7999.807276	13.870439	-0.061558	4.815295
303.682283	8000.098013	13.875443	-0.061534	4.815380
303.598258	8000.177860	13.880448	-0.061518	4.815404
303.580459	7999.922070	13.885453	-0.061514	4.815329
303.701349	8000.004251	13.890458	-0.061537	4.815353
303.809721	8000.017808	13.895463	-0.061557	4.815356
303.667775	8000.044311	13.900467	-0.061531	4.815365
303.626182	8000.112035	13.905472	-0.061523	4.815385
303.553968	8000.036003	13.910477	-0.061509	4.815363
303.518513	8000.116657	13.915482	-0.061503	4.815386
303.631727	7999.914356	13.920487	-0.061524	4.815327
303.733898	8000.112748	13.925491	-0.061543	4.815384
303.658545	7999.983213	13.930496	-0.061529	4.815347
303.695527	7999.929306	13.935501	-0.061536	4.815331
303.749555	8000.094829	13.940506	-0.061546	4.815379
303.743466	8000.168488	13.945511	-0.061545	4.815400
303.639057	8000.189201	13.950515	-0.061525	4.815407
303.695230	8000.086438	13.955520	-0.061536	4.815377
303.741201	8000.024128	13.960525	-0.061544	4.815358
303.707362	8000.077014	13.965530	-0.061538	4.815374
303.784253	7999.938249	13.970535	-0.061552	4.815333
303.957941	8000.077966	13.975539	-0.061584	4.815373
303.850197	8000.033414	13.980544	-0.061564	4.815360
303.789087	8000.033466	13.985549	-0.061553	4.815361
303.797859	8000.112716	13.990554	-0.061555	4.815384
303.667934	8000.133005	13.995559	-0.061530	4.815390
303.586439	8000.118822	14.000563	-0.061515	4.815387
303.640108	7999.960429	14.005568	-0.061525	4.815340
303.717706	7999.918956	14.010573	-0.061539	4.815328
303.727452	8000.109399	14.015578	-0.061541	4.815383
303.791959	7999.930875	14.020583	-0.061553	4.815331
303.770893	8000.024596	14.025587	-0.061549	4.815358
303.742723	7999.932192	14.030592	-0.061544	4.815331
303.894331	7999.831014	14.035597	-0.061572	4.815301
303.970919	8000.160471	14.040602	-0.061587	4.815397
303.691133	7999.815877	14.045607	-0.061534	4.815298
303.748826	8000.057359	14.050611	-0.061545	4.815368
303.829455	7999.935760	14.055616	-0.061560	4.815332
303.884292	7999.990120	14.060621	-0.061570	4.815348
303.803894	8000.156618	14.065626	-0.061555	4.815397
303.752211	8000.083064	14.070631	-0.061546	4.815375
303.803968	8000.164098	14.075635	-0.061555	4.815399
303.816198	8000.131160	14.080640	-0.061558	4.815389
303.523295	7999.859042	14.085645	-0.061503	4.815311
303.702900	8000.134619	14.090650	-0.061537	4.815391
303.874448	7999.905491	14.095655	-0.061568	4.815323
303.868703	7999.963120	14.100659	-0.061567	4.815340
304.001348	8000.062602	14.105664	-0.061592	4.815368
303.974795	8000.024743	14.110669	-0.061587	4.815357
303.842161	8000.160441	14.115674	-0.061562	4.815398
303.936645	7999.942861	14.120679	-0.061580	4.815334
303.838459	8000.049198	14.125683	-0.061562	4.815365
303.868334	8000.094591	14.130688	-0.061567	4.815378
303.858858	7999.930873	14.135693	-0.061565	4.815331
303.716362	8000.084580	14.140698	-0.061539	4.815376
303.882412	8000.101233	14.145703	-0.061570	4.815380
303.722357	8000.152023	14.150707	-0.061540	4.815396
303.709389	8000.102631	14.155712	-0.061537	4.815381
303.884679	7999.919533	14.160717	-0.061570	4.815327
303.720784	8000.094265	14.165722	-0.061539	4.815379
303.685964	8000.045579	14.170727	-0.061533	4.815365
303.746063	8000.041230	14.175731	-0.061544	4.815363
303.803224	7999.978037	14.180736	-0.061555	4.815345
303.900193	7999.933678	14.185741	-0.061573	4.815331
303.874823	8000.089331	14.190746	-0.061568	4.815377
303.931299	7999.944881	14.195751	-0.061578	4.815334
303.839996	8000.001089	14.200755	-0.061561	4.815351
303.846844	8000.083515	14.205760	-0.061563	4.815375
303.945531	8000.087291	14.210765	-0.061581	4.815376
303.853710	8000.081487	14.215770	-0.061564	4.815375
303.801878	7999.945929	14.220775	-0.061554	4.815335
303.724608	8000.146687	14.225779	-0.061540	4.815394
303.727602	8000.043040	14.230784	-0.061540	4.815364
303.966685	8000.114358	14.235789	-0.061585	4.815384
303.884715	8000.168583	14.240794	-0.061570	4.815400
303.942287	8000.100052	14.245799	-0.061580	4.815380
303.741600	7999.454251	14.250803	-0.061543	4.815192
303.630221	7996.286420	14.255808	-0.061520	4.814267
303.945501	7990.717862	14.260813	-0.061575	4.812639
303.749785	7983.943439	14.265818	-0.061534	4.810660
303.589085	7976.670711	14.270823	-0.061499	4.808534
303.694610	7969.039503	14.275827	-0.061514	4.806301
303.800465	7961.209184	14.280832	-0.061528	4.804009
303.704141	7953.343198	14.285837	-0.061505	4.801706
303.512719	7945.371965	14.290842	-0.061465	4.799372
303.869780	7937.447049	14.295847	-0.061526	4.797047
303.824632	7929.413413	14.300851	-0.061512	4.794692
303.614604	7921.361112	14.305856	-0.061468	4.792330
303.633095	7913.386366	14.310861	-0.061466	4.789990
303.712622	7905.361128	14.315866	-0.061476	4.787632
303.656083	7897.378266	14.320871	-0.061460	4.785287
303.472951	7889.441117	14.325875	-0.061421	4.782955
303.475453	7881.378872	14.330880	-0.061416	4.780584
303.572991	7873.417388	14.335885	-0.061429	4.778240
303.442493	7865.375100	14.340890	-0.061399	4.775873
303.512457	7857.394598	14.345895	-0.061407	4.773523
303.388777	7849.395376	14.350899	-0.061379	4.771166
303.193342	7841.335728	14.355904	-0.061337	4.768790
303.167701	7833.357440	14.360909	-0.061327	4.766437
303.304786	7825.347052	14.365914	-0.061347	4.764072
303.165617	7817.409111	14.370919	-0.061316	4.761729
303.260156	7809.391307	14.375923	-0.061329	4.759360
303.125380	7801.381097	14.380928	-0.061298	4.756993
303.298119	7793.371116	14.385933	-0.061325	4.754623
303.020806	7785.306131	14.390938	-0.061268	4.752238
303.192486	7777.269327	14.395943	-0.061295	4.749859
303.081236	7769.356679	14.400947	-0.061269	4.747516
302.991645	7761.265991	14.405952	-0.061247	4.745119
303.112810	7753.395401	14.410957	-0.061264	4.742785
302.804637	7745.300021	14.415962	-0.061202	4.740385
302.823118	7737.320548	14.420967	-0.061200	4.738017
302.955640	7729.371443	14.425971	-0.061219	4.735656
302.791860	7721.272035	14.430976	-0.061184	4.733251
302.805580	7713.305602	14.435981	-0.061181	4.730883
302.685684	7705.295711	14.440986	-0.061153	4.728501
302.619373	7697.290407	14.445991	-0.061136	4.726120
302.751303	7689.338160	14.450995	-0.061155	4.723752
302.634552	7681.290177	14.456000	-0.061128	4.721356
302.826908	7673.311873	14.461005	-0.061159	4.718978
302.825160	7665.341110	14.466010	-0.061153	4.716602
302.481699	7657.267932	14.471015	-0.061084	4.714195
302.316805	7649.262178	14.476019	-0.061048	4.711806
302.398244	7641.259371	14.481024	-0.061058	4.709417
302.437486	7633.284309	14.486029	-0.061060	4.707034
302.337784	7625.275679	14.491034	-0.061036	4.704641
302.324734	7617.330260	14.496039	-0.061029	4.702265
302.365876	7609.283888	14.501043	-0.061031	4.699858
302.400995	7601.311453	14.506048	-0.061032	4.697471
302.263960	7593.287706	14.511053	-0.061002	4.695069
302.340046	7585.242444	14.516058	-0.061011	4.692658
302.319239	7577.245447	14.521063	-0.061001	4.690261
302.299822	7569.300431	14.526067	-0.060993	4.687878
302.031122	7561.199890	14.531072	-0.060937	4.685447
302.360800	7553.313994	14.536077	-0.060994	4.683079
302.183160	7545.252500	14.541082	-0.060955	4.680657
302.163282	7537.296837	14.546087	-0.060946	4.678266
302.203179	7529.284332	14.551091	-0.060948	4.675857
302.011378	7521.204247	14.556096	-0.060907	4.673426
302.149575	7513.182918	14.561101	-0.060928	4.671011
301.975342	7505.180827	14.566106	-0.060890	4.668601
302.026312	7497.200515	14.571111	-0.060895	4.666196
301.926804	7489.241267	14.576115	-0.060871	4.663797
301.834601	7481.215832	14.581120	-0.060848	4.661376
301.956048	7473.234732	14.586125	-0.060866	4.658967
301.677796	7465.258325	14.591130	-0.060809	4.656559
301.652991	7457.220922	14.596135	-0.060799	4.654130
301.747270	7449.172634	14.601139	-0.060811	4.651697
301.484338	7441.130527	14.606144	-0.060757	4.649265
301.709953	7433.245768	14.611149	-0.060794	4.646879
301.703857	7425.184979	14.616154	-0.060787	4.644439
301.609827	7417.232285	14.621159	-0.060765	4.642030
301.474555	7409.229087	14.626163	-0.060734	4.639604
301.636535	7401.261642	14.631168	-0.060759	4.637188
301.567949	7393.210409	14.636173	-0.060741	4.634745
301.541414	7385.165584	14.641178	-0.060731	4.632303
301.453214	7377.156784	14.646183	-0.060709	4.629871
301.663232	7369.207071	14.651187	-0.060743	4.627455
301.448393	7361.152134	14.656192	-0.060698	4.625006
301.247947	7353.244188	14.661197	-0.060655	4.622601
301.276060	7345.177562	14.666202	-0.060655	4.620146
301.360103	7337.194173	14.671207	-0.060666	4.617715
301.308435	7329.159597	14.676211	-0.060651	4.615267
301.214497	7321.150807	14.681216	-0.060628	4.612825
301.324060	7313.144250	14.686221	-0.060643	4.610383
301.031885	7305.156307	14.691226	-0.060584	4.607946
301.187902	7297.111195	14.696231	-0.060607	4.605489
301.227192	7289.219561	14.701235	-0.060610	4.603078
301.128620	7281.157547	14.706240	-0.060586	4.600614
301.116411	7273.203915	14.711245	-0.060578	4.598182
301.177292	7265.161592	14.716250	-0.060585	4.595721
301.145688	7257.098202	14.721255	-0.060573	4.593252
301.171294	7249.089007	14.726259	-0.060573	4.590799
300.903594	7241.084609	14.731264	-0.060518	4.588346
301.062219	7233.110234	14.736269	-0.060542	4.585901
300.914376	7225.135632	14.741274	-0.060509	4.583454
300.803478	7217.189669	14.746279	-0.060484	4.581015
300.858513	7209.140865	14.751283	-0.060489	4.578543
300.718094	7201.111149	14.756288	-0.060457	4.576075
300.683826	7193.097698	14.761293	-0.060446	4.573611
300.624326	7185.077505	14.766298	-0.060429	4.571144
300.879336	7177.072799	14.771303	-0.060471	4.568680
300.834346	7169.136210	14.776307	-0.060458	4.566236
300.630673	7161.139655	14.781312	-0.060415	4.563772
300.704468	7153.157562	14.786317	-0.060423	4.561311
300.574547	7145.129997	14.791322	-0.060394	4.558835
300.305137	7137.165094	14.796327	-0.060338	4.556376
300.532643	7129.121520	14.801331	-0.060376	4.553893
300.500700	7121.050129	14.806336	-0.060364	4.551399
300.500802	7113.112260	14.811341	-0.060359	4.548945
300.334096	7105.092745	14.816346	-0.060323	4.546464
300.412505	7097.087487	14.821351	-0.060332	4.543987
300.394581	7089.142535	14.826355	-0.060324	4.541527
300.220034	7081.103052	14.831360	-0.060286	4.539036
300.413389	7073.138408	14.836365	-0.060317	4.536567
300.324728	7065.104257	14.841370	-0.060295	4.534075
300.394130	7057.052462	14.846375	-0.060303	4.531577
300.080687	7049.077910	14.851379	-0.060239	4.529100
300.078578	7041.075653	14.856384	-0.060233	4.526614
299.970284	7033.096598	14.861389	-0.060208	4.524133
299.953201	7025.143409	14.866394	-0.060200	4.521660
299.963259	7017.093089	14.871399	-0.060196	4.519155
300.059678	7009.151857	14.876403	-0.060209	4.516683
299.989946	7001.075937	14.881408	-0.060191	4.514166
299.958354	6992.994246	14.886413	-0.060179	4.511647
300.037144	6984.977258	14.891418	-0.060189	4.509147
299.901323	6977.033458	14.896423	-0.060158	4.506668
299.956961	6969.074498	14.901427	-0.060164	4.504183
299.814265	6961.096634	14.906432	-0.060132	4.501691
299.705613	6953.070032	14.911437	-0.060106	4.499182
299.802487	6945.081052	14.916442	-0.060119	4.496683
299.792935	6937.034616	14.921447	-0.060112	4.494165
299.894787	6929.060447	14.926451	-0.060126	4.491669
299.662966	6920.992230	14.931456	-0.060077	4.489141
299.636961	6913.058098	14.936461	-0.060067	4.486654
299.579473	6905.047090	14.941466	-0.060051	4.484141
299.723948	6897.058456	14.946471	-0.060073	4.481635
299.677104	6889.060307	14.951475	-0.060059	4.479124
299.628078	6881.056757	14.956480	-0.060045	4.476609
299.593352	6873.069494	14.961485	-0.060033	4.474098
299.459589	6865.009415	14.966490	-0.060003	4.471563
299.632994	6856.981315	14.971495	-0.060030	4.469037
299.674340	6849.033527	14.976499	-0.060032	4.466535
299.450866	6841.050616	14.981504	-0.059986	4.464019
299.356316	6833.037135	14.986509	-0.059963	4.461493
299.256711	6825.053037	14.991514	-0.059939	4.458974
299.159227	6817.017099	14.996519	-0.059916	4.456438
299.217541	6809.057023	15.001523	-0.059921	4.453925
299.208176	6800.971863	15.006528	-0.059914	4.451371
299.271616	6792.984234	15.011533	-0.059921	4.448846
299.022144	6784.981448	15.016538	-0.059869	4.446314
299.083290	6777.020710	15.021543	-0.059875	4.443794
299.237462	6769.015931	15.026547	-0.059899	4.441260
298.826745	6761.011412	15.031552	-0.059817	4.438722
299.091175	6753.039881	15.036557	-0.059861	4.436196
299.073680	6744.972380	15.041562	-0.059852	4.433637
298.852613	6736.937965	15.046567	-0.059806	4.431086
298.915239	6728.995655	15.051571	-0.059813	4.428564
298.828451	6720.935252	15.056576	-0.059791	4.426003
298.707297	6712.970373	15.061581	-0.059763	4.423470
298.640405	6704.951426	15.066586	-0.059746	4.420919
298.632847	6696.971555	15.071591	-0.059739	4.418378
298.894791	6688.999067	15.076595	-0.059783	4.415841
298.707558	6680.953720	15.081600	-0.059742	4.413276
298.691509	6672.922223	15.086605	-0.059734	4.410715
298.611447	6664.960977	15.091610	-0.059714	4.408174
298.451781	6656.936209	15.096615	-0.059679	4.405612
298.452654	6649.002515	15.101619	-0.059674	4.403078
298.458135	6640.964923	15.106624	-0.059670	4.400509
298.430047	6633.072151	15.111629	-0.059659	4.397985
298.512296	6624.980174	15.116634	-0.059669	4.395396
298.462067	6616.923447	15.121639	-0.059655	4.392816
298.594006	6608.968721	15.126643	-0.059674	4.390269
298.306556	6600.978097	15.131648	-0.059615	4.387706
298.397287	6592.970092	15.136653	-0.059627	4.385138
298.295986	6584.946797	15.141658	-0.059603	4.382563
298.388159	6576.923842	15.146663	-0.059615	4.379987
298.443893	6569.012121	15.151667	-0.059620	4.377446
298.264975	6560.993726	15.156672	-0.059581	4.374867
298.352091	6552.978148	15.161677	-0.059592	4.372289
298.289418	6544.951635	15.166682	-0.059576	4.369705
298.077031	6537.004434	15.171687	-0.059531	4.367145
298.091402	6528.986973	15.176691	-0.059528	4.364561
297.907114	6520.998403	15.181696	-0.059489	4.361984
298.070948	6512.987568	15.186701	-0.059514	4.359401
298.116499	6505.043685	15.191706	-0.059517	4.356837
298.054191	6496.957798	15.196711	-0.059500	4.354224
297.744950	6488.890420	15.201715	-0.059437	4.351615
297.747585	6480.865152	15.206720	-0.059433	4.349020
297.881218	6472.920140	15.211725	-0.059452	4.346450
297.758442	6464.939747	15.216730	-0.059424	4.343865
297.551947	6456.948558	15.221735	-0.059381	4.341275
297.833534	6448.970299	15.226739	-0.059428	4.338690
297.797037	6440.935095	15.231744	-0.059416	4.336084
297.694311	6432.936931	15.236749	-0.059391	4.333487
297.525413	6424.945035	15.241754	-0.059355	4.330891
297.591562	6416.909680	15.246759	-0.059362	4.328280
297.691378	6408.940811	15.251763	-0.059375	4.325690
297.653592	6400.951904	15.256768	-0.059363	4.323090
297.675850	6392.941559	15.261773	-0.059362	4.320483
297.585347	6384.976912	15.266778	-0.059340	4.317888
297.536641	6376.956779	15.271783	-0.059325	4.315273
297.782962	6368.956794	15.276787	-0.059366	4.312666
297.536743	6360.907884	15.281792	-0.059315	4.310038
297.431231	6352.912333	15.286797	-0.059290	4.307426
297.421214	6344.908933	15.291802	-0.059283	4.304811
297.593793	6336.929955	15.296807	-0.059310	4.302204
297.376140	6328.915446	15.301811	-0.059264	4.299581
297.312723	6320.944170	15.306816	-0.059247	4.296971
297.413632	6312.917566	15.311821	-0.059261	4.294343
297.068815	6304.924826	15.316826	-0.059191	4.291721
297.106936	6296.910556	15.321831	-0.059193	4.289093
297.149122	6288.932478	15.326835	-0.059196	4.286475
296.906024	6280.942635	15.331840	-0.059145	4.283850
297.007452	6272.902562	15.336845	-0.059159	4.281210
296.767529	6264.955837	15.341850	-0.059109	4.278595
296.759895	6256.915143	15.346855	-0.059102	4.275950
296.729975	6248.932164	15.351859	-0.059091	4.273322
296.676214	6240.866603	15.356864	-0.059076	4.270666
296.830843	6232.873559	15.361869	-0.059100	4.268033
296.700556	6224.860726	15.366874	-0.059070	4.265389
296.606225	6216.859533	15.371879	-0.059047	4.262748
296.602084	6208.906305	15.376883	-0.059041	4.260123
296.817956	6200.893489	15.381888	-0.059076	4.257477
296.534703	6192.946327	15.386893	-0.059018	4.254848
296.612489	6184.886769	15.391898	-0.059028	4.252182
296.521010	6176.849158	15.396903	-0.059005	4.249521
296.500764	6168.939042	15.401907	-0.058996	4.246901
296.300483	6160.901352	15.406912	-0.058954	4.244236
296.367721	6152.921514	15.411917	-0.058961	4.241590
296.416709	6144.931163	15.416922	-0.058965	4.238939
296.407347	6136.927721	15.421927	-0.058958	4.236282
296.432900	6128.896372	15.426931	-0.058958	4.233614
296.554529	6120.810979	15.431936	-0.058975	4.230927
296.460045	6112.890832	15.436941	-0.058952	4.228291
296.223168	6104.897326	15.441946	-0.058903	4.225628
296.359248	6096.934518	15.446951	-0.058923	4.222977
296.530665	6088.912873	15.451955	-0.058950	4.220305
296.362450	6080.965343	15.456960	-0.058913	4.217653
296.424217	6072.916841	15.461965	-0.058919	4.214968
296.125138	6064.947919	15.466970	-0.058858	4.212304
295.947836	6056.894529	15.471975	-0.058820	4.209611
296.106333	6048.941567	15.476979	-0.058844	4.206954
295.969931	6040.909376	15.481984	-0.058814	4.204265
295.974854	6032.948856	15.486989	-0.058810	4.201600
295.930442	6024.989342	15.491994	-0.058796	4.198933
296.136616	6016.933003	15.496999	-0.058829	4.196235
296.131783	6008.893088	15.502003	-0.058823	4.193538
295.723506	6000.820038	15.507008	-0.058742	4.190824
295.913727	5992.867994	15.512013	-0.058772	4.188156
295.982315	5984.861712	15.517018	-0.058779	4.185466
295.999579	5976.870571	15.522023	-0.058777	4.182779
295.963461	5968.914128	15.527027	-0.058765	4.180101
295.761764	5960.914471	15.532032	-0.058723	4.177405
295.774276	5952.888926	15.537037	-0.058720	4.174701
295.646988	5944.910244	15.542042	-0.058691	4.172010
295.598824	5936.817573	15.547047	-0.058677	4.169279
295.830809	5928.939014	15.552051	-0.058715	4.166622
295.628114	5920.910057	15.557056	-0.058672	4.163907
295.508847	5912.929761	15.562061	-0.058644	4.161208
295.604492	5904.925224	15.567066	-0.058657	4.158502
295.382510	5896.912790	15.572071	-0.058610	4.155787
295.442787	5888.893186	15.577075	-0.058616	4.153072
295.507938	5880.865750	15.582080	-0.058623	4.150352
295.392173	5872.858151	15.587085	-0.058596	4.147635
295.255766	5864.872213	15.592090	-0.058566	4.144923
295.212670	5856.866216	15.597095	-0.058552	4.142204
295.384260	5848.907482	15.602099	-0.058579	4.139501
295.155553	5840.907581	15.607104	-0.058531	4.136778
295.235540	5832.878132	15.612109	-0.058541	4.134047
295.280251	5824.867153	15.617114	-0.058544	4.131320
294.999271	5816.869591	15.622119	-0.058486	4.128592
295.033631	5808.859542	15.627123	-0.058488	4.125861
295.187800	5800.870526	15.632128	-0.058511	4.123138
295.200079	5792.889215	15.637133	-0.058508	4.120413
294.985525	5784.932545	15.642138	-0.058463	4.117692
295.145047	5776.881491	15.647143	-0.058487	4.114942
294.912383	5768.896961	15.652147	-0.058439	4.112208
294.628614	5760.865061	15.657152	-0.058381	4.109455
294.706420	5752.882405	15.662157	-0.058390	4.106721
294.744998	5744.864644	15.667162	-0.058392	4.103974
294.599093	5736.852919	15.672167	-0.058360	4.101224
294.698108	5728.903616	15.677171	-0.058373	4.098497
294.650322	5720.852553	15.682176	-0.058359	4.095731
294.732609	5712.884551	15.687181	-0.058369	4.092994
294.590787	5704.858891	15.692186	-0.058337	4.090232
294.422705	5696.895972	15.697191	-0.058301	4.087489
294.502716	5688.926902	15.702195	-0.058310	4.084746
294.485684	5680.951600	15.707200	-0.058302	4.081997
294.494285	5672.928174	15.712205	-0.058298	4.079230
294.618838	5664.987869	15.717210	-0.058316	4.076492
294.443596	5656.922079	15.722215	-0.058278	4.073704
294.336401	5648.928693	15.727219	-0.058253	4.070941
294.270128	5640.897612	15.732224	-0.058236	4.068163
294.276247	5632.887144	15.737229	-0.058231	4.065391
294.100110	5624.949985	15.742234	-0.058193	4.062640
294.158527	5616.900561	15.747239	-0.058199	4.059852
294.384676	5608.960438	15.752243	-0.058236	4.057102
294.394947	5600.923927	15.757248	-0.058233	4.054314
294.213913	5592.918896	15.762253	-0.058194	4.051532
294.178068	5584.929537	15.767258	-0.058182	4.048755
294.205396	5576.922378	15.772263	-0.058182	4.045972
294.142165	5568.995416	15.777267	-0.058165	4.043213
294.242109	5560.922653	15.782272	-0.058178	4.040404
294.067662	5552.966598	15.787277	-0.058140	4.037629
294.017777	5544.939146	15.792282	-0.058126	4.034830
293.858197	5536.829876	15.797287	-0.058091	4.031998
294.097172	5528.840557	15.802291	-0.058130	4.029212
293.700749	5520.891397	15.807296	-0.058051	4.026429
293.663465	5512.893864	15.812301	-0.058039	4.023632
293.852602	5504.907163	15.817306	-0.058069	4.020841
293.878775	5496.923299	15.822311	-0.058068	4.018046
293.792556	5488.909866	15.827315	-0.058047	4.015237
293.804115	5480.887063	15.832320	-0.058044	4.012425
293.792464	5472.878929	15.837325	-0.058037	4.009615
293.700485	5464.961796	15.842330	-0.058014	4.006834
293.375961	5456.897213	15.847335	-0.057949	4.003995
293.484636	5448.942319	15.852339	-0.057964	4.001200
293.370540	5440.914342	15.857344	-0.057937	3.998374
293.300818	5432.925533	15.862349	-0.057919	3.995560
293.415686	5424.915345	15.867354	-0.057935	3.992740
293.360126	5416.854872	15.872359	-0.057919	3.989897
293.404899	5408.908766	15.877363	-0.057923	3.987094
293.205351	5400.878787	15.882368	-0.057880	3.984255
293.366484	5392.943840	15.887373	-0.057905	3.981454
293.177943	5384.950424	15.892378	-0.057865	3.978625
293.091060	5376.939493	15.897383	-0.057843	3.975789
293.260155	5368.915217	15.902387	-0.057870	3.972950
293.210176	5360.891998	15.907392	-0.057855	3.970106
293.096754	5352.940935	15.912397	-0.057829	3.967285
293.268370	5344.930107	15.917402	-0.057855	3.964445
293.303134	5336.969294	15.922407	-0.057857	3.961619
293.126756	5328.981267	15.927411	-0.057819	3.958777
292.924398	5320.975738	15.932416	-0.057776	3.955927
293.149297	5312.936083	15.937421	-0.057812	3.953070
292.983377	5304.931674	15.942426	-0.057776	3.950216
292.908784	5296.919911	15.947431	-0.057757	3.947359
293.067162	5288.941069	15.952435	-0.057781	3.944516
292.948649	5280.985043	15.957440	-0.057754	3.941675
292.703451	5272.988643	15.962445	-0.057703	3.938814
292.866910	5264.980513	15.967450	-0.057728	3.935955
292.654070	5256.990769	15.972455	-0.057683	3.933093
292.820304	5248.967937	15.977459	-0.057709	3.930225
292.622236	5241.009256	15.982464	-0.057667	3.927370
292.482879	5232.968176	15.987469	-0.057636	3.924485
292.728505	5225.017133	15.992474	-0.057676	3.921637
292.637325	5216.968898	15.997479	-0.057654	3.918746
292.661802	5209.020653	16.002483	-0.057653	3.915891
292.705051	5200.978284	16.007488	-0.057656	3.913000
292.570204	5192.950991	16.012493	-0.057626	3.910110
292.421922	5184.997130	16.017498	-0.057593	3.907243
292.323002	5176.952217	16.022503	-0.057569	3.904343
292.441129	5169.013707	16.027507	-0.057586	3.901482
292.442761	5160.997969	16.032512	-0.057581	3.898590
292.254170	5152.996408	16.037517	-0.057541	3.895696
292.416248	5145.008374	16.042522	-0.057566	3.892813
292.120277	5136.959730	16.047527	-0.057505	3.889896
292.349684	5128.986903	16.052531	-0.057543	3.887015
292.197526	5120.995348	16.057536	-0.057509	3.884117
292.197560	5113.009468	16.062541	-0.057504	3.881223
292.083284	5105.033084	16.067546	-0.057478	3.878327
291.998947	5097.020701	16.072551	-0.057457	3.875417
292.178173	5088.796597	16.077555	-0.057485	3.872432
291.966678	5080.811898	16.082560	-0.057440	3.869525
291.871413	5072.882743	16.087565	-0.057417	3.866638
291.778268	5064.924301	16.092570	-0.057395	3.863738
291.665476	5056.950687	16.097575	-0.057368	3.860831
291.842181	5048.982667	16.102579	-0.057396	3.857928
291.890093	5040.948132	16.107584	-0.057400	3.854997
291.741425	5032.962164	16.112589	-0.057367	3.852077
291.716780	5024.983989	16.117594	-0.057357	3.849161
291.641827	5016.970309	16.122599	-0.057338	3.846228
291.701936	5009.028563	16.127603	-0.057344	3.843322
291.529407	5001.048752	16.132608	-0.057307	3.840395
291.617489	4993.041737	16.137613	-0.057318	3.837461
291.750983	4985.039105	16.142618	-0.057337	3.834528
291.677186	4976.994777	16.147623	-0.057318	3.831573
291.458097	4969.031184	16.152627	-0.057272	3.828642
291.598655	4961.009179	16.157632	-0.057293	3.825695
291.568296	4953.061578	16.162637	-0.057282	3.822769
291.496807	4945.083463	16.167642	-0.057264	3.819829
291.310796	4937.078324	16.172647	-0.057224	3.816874
291.425640	4929.074793	16.177651	-0.057240	3.813924
291.146837	4921.061326	16.182656	-0.057183	3.810960
291.150759	4913.072422	16.187661	-0.057178	3.808008
291.177138	4905.067308	16.192666	-0.057178	3.805049
291.053626	4897.087306	16.197671	-0.057150	3.802094
291.221055	4889.104919	16.202675	-0.057176	3.799141
290.987541	4881.123653	16.207680	-0.057127	3.796178
291.073745	4873.084402	16.212685	-0.057138	3.793198
290.978562	4865.057144	16.217690	-0.057115	3.790216
290.910255	4857.068256	16.222695	-0.057097	3.787247
290.968657	4849.060483	16.227699	-0.057103	3.784271
290.752832	4841.137470	16.232704	-0.057057	3.781318
290.988606	4833.089706	16.237709	-0.057096	3.778327
290.984813	4825.096986	16.242714	-0.057090	3.775348
290.874846	4817.086876	16.247719	-0.057064	3.772358
290.891774	4809.072133	16.252723	-0.057062	3.769367
290.860890	4801.095063	16.257728	-0.057051	3.766386
290.776335	4793.092543	16.262733	-0.057030	3.763393
290.772122	4785.137391	16.267738	-0.057024	3.760416
290.716348	4777.130872	16.272743	-0.057009	3.757417
290.780052	4769.112591	16.277747	-0.057015	3.754413
290.554585	4761.115244	16.282752	-0.056968	3.751409
290.663962	4753.072060	16.287757	-0.056983	3.748392
290.752499	4745.077313	16.292762	-0.056994	3.745391
290.456210	4737.112113	16.297767	-0.056934	3.742390
290.501313	4729.108856	16.302771	-0.056937	3.739379
290.555959	4721.141267	16.307776	-0.056942	3.736380
290.439786	4713.108002	16.312781	-0.056915	3.733350
290.465949	4705.126938	16.317786	-0.056915	3.730341
290.359593	4697.140861	16.322791	-0.056890	3.727323
290.426628	4689.099072	16.327795	-0.056897	3.724287
290.342684	4681.176613	16.332800	-0.056876	3.721290
290.301338	4673.186932	16.337805	-0.056863	3.718265
290.372947	4665.193237	16.342810	-0.056871	3.715240
290.350477	4657.102570	16.347815	-0.056862	3.712173
290.290415	4649.100831	16.352819	-0.056846	3.709136
290.183861	4641.111152	16.357824	-0.056820	3.706100
290.164980	4633.155238	16.362829	-0.056812	3.703077
290.058125	4625.191864	16.367834	-0.056787	3.700046
289.812743	4617.217871	16.372839	-0.056736	3.697005
289.970447	4609.192212	16.377843	-0.056760	3.693952
289.836630	4601.170162	16.382848	-0.056730	3.690891
289.779661	4593.212755	16.387853	-0.056714	3.687853
289.902527	4585.178137	16.392858	-0.056731	3.684788
289.783694	4577.215978	16.397863	-0.056704	3.681742
289.923487	4569.225336	16.402867	-0.056725	3.678690
289.866219	4561.248693	16.407872	-0.056709	3.675635
289.648436	4553.234049	16.412877	-0.056663	3.672559
289.756843	4545.205991	16.417882	-0.056678	3.669483
289.648785	4537.219499	16.422887	-0.056653	3.666416
289.617975	4529.236164	16.427891	-0.056642	3.663349
289.421891	4521.256905	16.432896	-0.056600	3.660276
289.499314	4513.256164	16.437901	-0.056609	3.657200
289.769200	4505.260390	16.442906	-0.056654	3.654128
289.444389	4497.247795	16.447911	-0.056589	3.651032
289.426130	4489.241418	16.452915	-0.056580	3.647943
289.376831	4481.256090	16.457920	-0.056566	3.644859
289.418175	4473.293931	16.462925	-0.056568	3.641784
289.443873	4465.288722	16.467930	-0.056568	3.638689
289.160213	4457.300418	16.472935	-0.056510	3.635590
289.190474	4449.248955	16.477939	-0.056510	3.632472
289.129487	4441.242134	16.482944	-0.056493	3.629367
289.057237	4433.271939	16.487949	-0.056475	3.626272
289.038772	4425.287147	16.492954	-0.056466	3.623171
288.971426	4417.278109	16.497959	-0.056448	3.620056
289.028194	4409.310592	16.502963	-0.056454	3.616958
289.169088	4401.304679	16.507968	-0.056475	3.613845
289.162183	4393.272811	16.512973	-0.056468	3.610714
289.035168	4385.335642	16.517978	-0.056439	3.607615
288.751648	4377.314954	16.522983	-0.056381	3.604476
288.841353	4369.368236	16.527987	-0.056393	3.601374
288.747158	4361.388005	16.532992	-0.056370	3.598251
288.552012	4353.365373	16.537997	-0.056328	3.595105
288.690986	4345.361699	16.543002	-0.056349	3.591974
288.854950	4337.313800	16.548007	-0.056374	3.588823
288.772866	4329.361449	16.553011	-0.056354	3.585700
288.550274	4321.396053	16.558016	-0.056307	3.582566
288.757449	4313.360482	16.563021	-0.056340	3.579413
288.698901	4305.420255	16.568026	-0.056324	3.576287
288.341840	4297.415287	16.573031	-0.056253	3.573124
288.373308	4289.393091	16.578035	-0.056253	3.569963
288.459614	4281.429340	16.583040	-0.056264	3.566824
288.565411	4273.398420	16.588045	-0.056278	3.563656
288.544821	4265.436831	16.593050	-0.056269	3.560509
288.363807	4257.448404	16.598055	-0.056230	3.557344
288.303146	4249.415683	16.603059	-0.056214	3.554162
288.382272	4241.325456	16.608064	-0.056223	3.550959
288.333503	4233.360614	16.613069	-0.056209	3.547798
288.301943	4225.367022	16.618074	-0.056198	3.544624
288.015544	4217.427983	16.623079	-0.056139	3.541461
288.118294	4209.444176	16.628083	-0.056153	3.538289
288.117748	4201.436852	16.633088	-0.056148	3.535102
288.003053	4193.430495	16.638093	-0.056121	3.531909
288.086086	4185.428986	16.643098	-0.056132	3.528721
288.197291	4177.387189	16.648103	-0.056147	3.525514
288.152693	4169.466070	16.653107	-0.056134	3.522349
287.876757	4161.516677	16.658112	-0.056077	3.519162
287.834588	4153.485000	16.663117	-0.056064	3.515946
287.893736	4145.488761	16.668122	-0.056070	3.512745
287.781846	4137.459236	16.673127	-0.056044	3.509522
287.907995	4129.489558	16.678131	-0.056062	3.506327
287.798251	4121.483166	16.683136	-0.056036	3.503108
287.721739	4113.495587	16.688141	-0.056017	3.499894
287.751604	4105.549774	16.693146	-0.056017	3.496698
287.850905	4097.503549	16.698151	-0.056030	3.493460
287.726003	4089.524035	16.703155	-0.056002	3.490239
287.645330	4081.557770	16.708160	-0.055982	3.487022
287.707387	4073.553712	16.713165	-0.055988	3.483791
287.766887	4065.598939	16.718170	-0.055994	3.480577
287.599320	4057.616176	16.723175	-0.055957	3.477341
287.613496	4049.594209	16.728179	-0.055955	3.474092
287.272188	4041.587116	16.733184	-0.055886	3.470835
287.362382	4033.568055	16.738189	-0.055898	3.467584
287.253750	4025.610715	16.743194	-0.055872	3.464348
287.208399	4017.635093	16.748199	-0.055858	3.461104
287.195153	4009.626066	16.753203	-0.055851	3.457844
287.092919	4001.637099	16.758208	-0.055826	3.454587
287.108622	3993.635528	16.763213	-0.055824	3.451325
287.203860	3985.627466	16.768218	-0.055837	3.448060
287.123247	3977.606772	16.773223	-0.055816	3.444781
286.962835	3969.652877	16.778227	-0.055781	3.441523
287.041925	3961.655137	16.783232	-0.055791	3.438253
287.048944	3953.657126	16.788237	-0.055787	3.434977
287.091460	3945.674507	16.793242	-0.055790	3.431705
287.022188	3937.647039	16.798247	-0.055771	3.428408
286.853637	3929.675717	16.803251	-0.055735	3.425127
286.698117	3921.723945	16.808256	-0.055701	3.421852
286.755623	3913.710026	16.813261	-0.055706	3.418555
286.924813	3905.711267	16.818266	-0.055732	3.415265
286.726693	3897.714947	16.823271	-0.055690	3.411960
286.642927	3889.711704	16.828275	-0.055669	3.408653
286.697501	3881.719884	16.833280	-0.055674	3.405353
286.579973	3873.774261	16.838285	-0.055647	3.402062
286.609657	3865.782647	16.843290	-0.055648	3.398754
286.617687	3857.780286	16.848295	-0.055644	3.395438
286.713976	3849.703877	16.853299	-0.055656	3.392091
286.659072	3841.733018	16.858304	-0.055641	3.388779
286.443585	3833.743719	16.863309	-0.055596	3.385451
286.668163	3825.773233	16.868314	-0.055632	3.382143
286.447022	3817.804699	16.873319	-0.055586	3.378816
286.518220	3809.801367	16.878323	-0.055594	3.375482
286.399890	3801.815292	16.883328	-0.055567	3.372145
286.192631	3793.825336	16.888333	-0.055523	3.368800
286.247471	3785.832232	16.893338	-0.055528	3.365460
286.269723	3777.861015	16.898343	-0.055527	3.362125
286.250178	3769.870006	16.903347	-0.055518	3.358776
286.269048	3761.876981	16.908352	-0.055516	3.355425
286.062708	3753.848903	16.913357	-0.055472	3.352047
286.316906	3745.851627	16.918362	-0.055515	3.348695
286.161951	3737.873171	16.923367	-0.055480	3.345334
286.087927	3729.908390	16.928371	-0.055461	3.341977
286.170286	3721.904743	16.933376	-0.055472	3.338607
286.069314	3713.922157	16.938381	-0.055448	3.335235
285.911345	3705.936418	16.943386	-0.055413	3.331856
285.790420	3697.920929	16.948391	-0.055385	3.328463
285.935484	3689.921315	16.953395	-0.055407	3.325083
285.804906	3681.991562	16.958400	-0.055377	3.321718
285.844850	3673.980572	16.963405	-0.055380	3.318323
285.926050	3666.008673	16.968410	-0.055390	3.314942
285.719538	3657.962386	16.973415	-0.055346	3.311514
285.599958	3649.989444	16.978419	-0.055318	3.308118
285.716977	3641.970750	16.983424	-0.055335	3.304708
285.581128	3634.020134	16.988429	-0.055304	3.301314
285.571375	3626.046035	16.993434	-0.055297	3.297911
285.388046	3618.037989	16.998439	-0.055258	3.294483
285.514092	3610.037639	17.003443	-0.055276	3.291067
285.515919	3602.026081	17.008448	-0.055271	3.287638
285.434663	3594.039103	17.013453	-0.055251	3.284213
285.460194	3586.126524	17.018458	-0.055251	3.280820
285.454098	3578.095626	17.023463	-0.055244	3.277371
285.497554	3570.083944	17.028467	-0.055247	3.273929
285.392029	3562.107250	17.033472	-0.055222	3.270493
285.212778	3554.116725	17.038477	-0.055183	3.267044
285.220555	3546.134320	17.043482	-0.055180	3.263602
285.222727	3538.151450	17.048487	-0.055175	3.260156
285.185957	3530.179144	17.053491	-0.055163	3.256710
285.053840	3522.180045	17.058496	-0.055133	3.253244
284.870193	3514.158248	17.063501	-0.055094	3.249763
284.902888	3506.197183	17.068506	-0.055094	3.246314
284.955510	3498.171545	17.073511	-0.055099	3.242833
284.893048	3490.211837	17.078515	-0.055082	3.239372
284.752594	3482.252116	17.083520	-0.055051	3.235905
284.649289	3474.180005	17.088525	-0.055026	3.232387
284.814224	3466.199151	17.093530	-0.055052	3.228915
284.732579	3458.181155	17.098535	-0.055031	3.225413
284.922857	3450.205066	17.103539	-0.055062	3.221937
284.757110	3442.263715	17.108544	-0.055025	3.218458
284.534659	3434.272916	17.113549	-0.054979	3.214951
284.633575	3426.284213	17.118554	-0.054992	3.211455
284.614262	3418.286861	17.123559	-0.054983	3.207945
284.571591	3410.279163	17.128563	-0.054970	3.204427
284.507241	3402.349761	17.133568	-0.054953	3.200938
284.363228	3394.366409	17.138573	-0.054921	3.197418
284.655201	3386.377394	17.143578	-0.054970	3.193911
284.466701	3378.342327	17.148583	-0.054930	3.190358
284.373063	3370.360247	17.153587	-0.054907	3.186829
284.488633	3362.366347	17.158592	-0.054923	3.183300
284.429219	3354.374053	17.163597	-0.054907	3.179761
284.535238	3346.421993	17.168602	-0.054921	3.176242
284.284907	3338.432784	17.173607	-0.054870	3.172687
284.317952	3330.423933	17.178611	-0.054870	3.169132
284.091412	3322.456147	17.183616	-0.054823	3.165581
284.131309	3314.466025	17.188621	-0.054825	3.162026
284.320617	3306.475283	17.193626	-0.054855	3.158474
283.934096	3298.526308	17.198631	-0.054778	3.154911
284.021810	3290.482342	17.203635	-0.054789	3.151323
283.729569	3282.513179	17.208640	-0.054730	3.147747
283.690635	3274.492907	17.213645	-0.054717	3.144156
283.696887	3266.534493	17.218650	-0.054713	3.140590
283.745179	3258.555953	17.223655	-0.054717	3.137013
283.556382	3250.568122	17.228659	-0.054676	3.133417
283.461486	3242.571286	17.233664	-0.054654	3.129817
283.531443	3234.577824	17.238669	-0.054661	3.126221
283.628085	3226.610272	17.243674	-0.054674	3.122635
283.396305	3218.627669	17.248679	-0.054626	3.119023
283.364398	3210.665669	17.253683	-0.054615	3.115425
283.474071	3202.627739	17.258688	-0.054630	3.111794
283.508831	3194.623143	17.263693	-0.054631	3.108172
283.568622	3186.637754	17.268698	-0.054637	3.104554
283.593442	3178.680957	17.273703	-0.054636	3.100944
283.567017	3170.724819	17.278707	-0.054626	3.097328
283.623469	3162.720278	17.283712	-0.054631	3.093690
283.356302	3154.690561	17.288717	-0.054576	3.090020
283.312672	3146.754725	17.293722	-0.054563	3.086400
283.235200	3138.764664	17.298727	-0.054543	3.082748
283.082781	3130.795111	17.303731	-0.054510	3.079099
283.302734	3122.821187	17.308736	-0.054546	3.075460
283.196254	3114.720863	17.313741	-0.054520	3.071744
282.983414	3106.768425	17.318746	-0.054476	3.068086
283.123291	3098.738649	17.323751	-0.054496	3.064405
283.072427	3090.803768	17.328755	-0.054482	3.060754
283.236365	3082.830635	17.333760	-0.054507	3.057092
283.078810	3074.839028	17.338765	-0.054473	3.053401
283.168177	3066.854103	17.343770	-0.054484	3.049720
282.999133	3058.904029	17.348775	-0.054447	3.046039
283.016244	3050.919496	17.353779	-0.054445	3.042346
283.052983	3042.925779	17.358784	-0.054447	3.038646
282.741459	3034.964386	17.363789	-0.054384	3.034939
282.867710	3026.958060	17.368794	-0.054402	3.031228
282.776808	3018.972635	17.373799	-0.054380	3.027511
282.765082	3010.970719	17.378803	-0.054372	3.023787
282.582911	3003.028589	17.383808	-0.054333	3.020077
282.481823	2995.034343	17.388813	-0.054309	3.016342
282.694202	2987.023911	17.393818	-0.054343	3.012610
282.499154	2979.048022	17.398823	-0.054302	3.008870
282.396118	2971.063823	17.403827	-0.054277	3.005126
282.504049	2963.119321	17.408832	-0.054292	3.001406
282.553808	2955.118311	17.413837	-0.054296	2.997652
282.383204	2947.157220	17.418842	-0.054259	2.993901
282.308821	2939.107846	17.423847	-0.054240	2.990109
282.314673	2931.129068	17.428851	-0.054236	2.986349
282.304400	2923.168663	17.433856	-0.054229	2.982592
282.100455	2915.190039	17.438861	-0.054186	2.978813
282.427857	2907.183459	17.443866	-0.054242	2.975042
282.148845	2899.229904	17.448871	-0.054184	2.971260
282.186772	2891.233625	17.453875	-0.054186	2.967470
282.156148	2883.256865	17.458880	-0.054175	2.963680
281.939721	2875.281408	17.463885	-0.054130	2.959877
281.876588	2867.333901	17.468890	-0.054113	2.956090
282.063866	2859.279301	17.473895	-0.054142	2.952260
282.014267	2851.297238	17.478899	-0.054128	2.948447
281.974272	2843.340808	17.483904	-0.054115	2.944643
281.900019	2835.381446	17.488909	-0.054096	2.940830
281.912767	2827.400863	17.493914	-0.054093	2.937006
281.735273	2819.409741	17.498919	-0.054055	2.933163
281.777599	2811.399396	17.503923	-0.054058	2.929316
281.931620	2803.430163	17.508928	-0.054081	2.925491
281.887916	2795.448201	17.513933	-0.054068	2.921643
281.758304	2787.512059	17.518938	-0.054039	2.917809
281.466507	2779.520883	17.523943	-0.053979	2.913934
281.617512	2771.410540	17.528947	-0.054002	2.910019
281.769316	2763.468782	17.533952	-0.054025	2.906181
281.690506	2755.516547	17.538957	-0.054005	2.902321
281.474488	2747.574030	17.543962	-0.053960	2.898453
281.634561	2739.560180	17.548967	-0.053984	2.894565
281.428367	2731.580320	17.553971	-0.053941	2.890669
281.375574	2723.619890	17.558976	-0.053926	2.886785
281.256708	2715.622591	17.563981	-0.053898	2.882874
281.150293	2707.675666	17.568986	-0.053873	2.878984
281.183477	2699.694637	17.573991	-0.053874	2.875079
281.294626	2691.691528	17.578995	-0.053890	2.871162
281.316770	2683.698446	17.584000	-0.053888	2.867240
281.015687	2675.748121	17.589005	-0.053827	2.863315
281.172201	2667.755515	17.594010	-0.053851	2.859390
281.218341	2659.785595	17.599015	-0.053854	2.855464
281.094123	2651.797787	17.604019	-0.053826	2.851515
281.052048	2643.821930	17.609024	-0.053813	2.847571
281.082551	2635.843258	17.614029	-0.053814	2.843624
281.105544	2627.877129	17.619034	-0.053813	2.839677
280.942664	2619.924944	17.624039	-0.053777	2.835721
280.661584	2611.933363	17.629043	-0.053719	2.831733
280.943070	2603.901618	17.634048	-0.053767	2.827752
280.735511	2595.922461	17.639053	-0.053723	2.823763
280.728139	2587.979305	17.644058	-0.053716	2.819798
280.732257	2580.009183	17.649063	-0.053712	2.815815
280.384152	2572.020314	17.654067	-0.053642	2.811796
280.504383	2564.034669	17.659072	-0.053659	2.807800
280.710430	2556.014397	17.664077	-0.053692	2.803786
280.859775	2548.064169	17.669082	-0.053715	2.799799
280.423921	2540.153114	17.674087	-0.053628	2.795791
280.572892	2532.114811	17.679091	-0.053651	2.791747
280.721940	2524.114634	17.684096	-0.053673	2.787717
280.439829	2516.155631	17.689101	-0.053616	2.783677
280.356971	2508.207352	17.694106	-0.053595	2.779647
280.272737	2500.255422	17.699111	-0.053574	2.775610
280.156417	2492.256799	17.704115	-0.053547	2.771542
280.139463	2484.289046	17.709120	-0.053539	2.767489
280.217690	2476.283242	17.714125	-0.053548	2.763416
280.225302	2468.332951	17.719130	-0.053544	2.759361
280.119415	2460.362472	17.724135	-0.053519	2.755284
280.025029	2452.301874	17.729139	-0.053497	2.751155
280.123857	2444.308606	17.734144	-0.053510	2.747065
279.998714	2436.353007	17.739149	-0.053481	2.742976
280.052405	2428.411272	17.744154	-0.053486	2.738898
279.938414	2420.435716	17.749159	-0.053460	2.734787
279.933925	2412.439861	17.754163	-0.053453	2.730666
279.854534	2404.496402	17.759168	-0.053433	2.726560
279.801209	2396.515986	17.764173	-0.053418	2.722432
279.686348	2388.571909	17.769178	-0.053392	2.718311
279.576706	2380.603820	17.774183	-0.053366	2.714173
279.729097	2372.569162	17.779187	-0.053389	2.710010
279.750784	2364.631988	17.784192	-0.053388	2.705883
279.550009	2356.668315	17.789197	-0.053345	2.701722
279.668453	2348.684055	17.794202	-0.053362	2.697564
279.429961	2340.732895	17.799207	-0.053313	2.693394
279.364717	2332.729789	17.804211	-0.053295	2.689201
279.508644	2324.747873	17.809216	-0.053317	2.685027
279.399712	2316.794002	17.814221	-0.053291	2.680844
279.446361	2308.843257	17.819226	-0.053295	2.676666
279.323731	2300.835979	17.824231	-0.053267	2.672442
279.384428	2292.838677	17.829235	-0.053273	2.668227
279.243422	2284.886781	17.834240	-0.053241	2.664017
278.993270	2276.936075	17.839245	-0.053190	2.659794
279.181948	2268.968119	17.844250	-0.053220	2.655584
279.095060	2260.973505	17.849255	-0.053198	2.651334
278.888282	2253.025797	17.854259	-0.053154	2.647095
279.065369	2245.046204	17.859264	-0.053182	2.642857
279.097401	2237.072265	17.864269	-0.053183	2.638606
278.941924	2229.123420	17.869274	-0.053149	2.634349
278.770626	2221.128542	17.874279	-0.053112	2.630060
278.873168	2213.129305	17.879283	-0.053126	2.625779
278.865149	2205.191288	17.884288	-0.053119	2.621517
278.617962	2197.224146	17.889293	-0.053068	2.617216
278.533804	2189.265665	17.894298	-0.053047	2.612924
278.495778	2181.270636	17.899303	-0.053034	2.608608
278.621457	2173.285236	17.904307	-0.053053	2.604301
278.598351	2165.353689	17.909312	-0.053043	2.600006
278.534811	2157.395139	17.914317	-0.053026	2.595687
278.461821	2149.269843	17.919322	-0.053007	2.591269
278.353580	2141.282975	17.924327	-0.052982	2.586916
278.531897	2133.326354	17.929331	-0.053010	2.582592
278.548778	2125.407214	17.934336	-0.053008	2.578271
278.454632	2117.457960	17.939341	-0.052985	2.573918
278.395329	2109.493899	17.944346	-0.052969	2.569552
278.405198	2101.534966	17.949351	-0.052965	2.565186
278.347203	2093.578846	17.954355	-0.052949	2.560809
278.084570	2085.676125	17.959360	-0.052895	2.556440
278.111136	2077.662472	17.964365	-0.052895	2.552023
278.303123	2069.662013	17.969370	-0.052925	2.547616
278.126986	2061.724870	17.974375	-0.052887	2.543212
277.946084	2053.779396	17.979379	-0.052849	2.538794
277.901713	2045.823152	17.984384	-0.052835	2.534373
277.953700	2037.814403	17.989389	-0.052840	2.529922
277.949421	2029.870565	17.994394	-0.052834	2.525494
277.903455	2021.913583	17.999399	-0.052820	2.521049
277.732551	2013.970781	18.004403	-0.052783	2.516595
277.720892	2005.987449	18.009408	-0.052775	2.512122
277.640549	1997.986878	18.014413	-0.052755	2.507626
277.807194	1990.003837	18.019418	-0.052781	2.503149
277.746672	1982.058733	18.024423	-0.052765	2.498670
277.507121	1974.118145	18.029427	-0.052715	2.494172
277.476128	1966.142140	18.034432	-0.052704	2.489661
277.373604	1958.191250	18.039437	-0.052679	2.485151
277.436774	1950.220978	18.044442	-0.052686	2.480633
277.303884	1942.293128	18.049447	-0.052656	2.476118
277.319333	1934.281904	18.054451	-0.052654	2.471557
277.277390	1926.335305	18.059456	-0.052641	2.467021
277.095077	1918.381280	18.064461	-0.052602	2.462461
277.163478	1910.413403	18.069466	-0.052609	2.457904
277.142555	1902.449656	18.074471	-0.052600	2.453334
276.916392	1894.486417	18.079475	-0.052553	2.448740
277.064553	1886.522419	18.084480	-0.052575	2.444166
276.919406	1878.578818	18.089485	-0.052543	2.439572
276.879106	1870.649408	18.094490	-0.052530	2.434986
276.988669	1862.575415	18.099495	-0.052545	2.430319
276.994570	1854.605000	18.104499	-0.052541	2.425695
277.051890	1846.674360	18.109504	-0.052547	2.421089
276.800302	1838.744523	18.114509	-0.052495	2.416452
276.879578	1830.761049	18.119514	-0.052504	2.411799
276.733091	1822.818378	18.124519	-0.052472	2.407144
276.582351	1814.870691	18.129523	-0.052438	2.402477
276.775197	1806.916939	18.134528	-0.052469	2.397824
276.655093	1798.958726	18.139533	-0.052441	2.393134
276.561961	1790.981875	18.144538	-0.052419	2.388427
276.457237	1783.030806	18.149543	-0.052394	2.383724
276.558532	1775.066034	18.154547	-0.052408	2.379021
276.497958	1767.143132	18.159552	-0.052391	2.374320
276.215521	1759.164939	18.164557	-0.052334	2.369559
276.371141	1751.203224	18.169562	-0.052357	2.364833
276.359418	1743.268097	18.174567	-0.052350	2.360100
276.128673	1735.341644	18.179571	-0.052302	2.355346
276.158032	1727.360500	18.184576	-0.052302	2.350570
276.180090	1719.362224	18.189581	-0.052301	2.345773
276.010959	1711.429543	18.194586	-0.052264	2.340991
276.044759	1703.482006	18.199591	-0.052265	2.336206
275.916453	1695.516951	18.204595	-0.052236	2.331387
276.215424	1687.534512	18.209600	-0.052287	2.326583
275.995239	1679.607471	18.214605	-0.052241	2.321760
275.826202	1671.685177	18.219610	-0.052204	2.316934
275.839842	1663.719166	18.224615	-0.052201	2.312087
275.633574	1655.760572	18.229619	-0.052158	2.307215
275.891874	1647.788907	18.234624	-0.052200	2.302364
275.811002	1639.834338	18.239629	-0.052180	2.297485
275.680174	1631.901289	18.244634	-0.052151	2.292605
275.666502	1623.946523	18.249639	-0.052143	2.287710
275.563019	1616.000417	18.254643	-0.052118	2.282803
275.522839	1608.081646	18.259648	-0.052106	2.277907
275.373688	1600.099021	18.264653	-0.052073	2.272952
275.570658	1592.074923	18.269658	-0.052104	2.267990
275.447284	1584.145491	18.274663	-0.052076	2.263049
275.253910	1576.222899	18.279667	-0.052035	2.258094
275.294125	1568.276357	18.284672	-0.052037	2.253135
275.319670	1560.299742	18.289677	-0.052037	2.248144
275.216616	1552.373149	18.294682	-0.052012	2.243162
275.138358	1544.450594	18.299687	-0.051993	2.238174
275.053705	1536.498632	18.304691	-0.051972	2.233155
275.151444	1528.516843	18.309696	-0.051985	2.228123
275.064202	1520.571047	18.314701	-0.051963	2.223085
274.918434	1512.669953	18.319706	-0.051931	2.218060
275.123875	1504.695568	18.324711	-0.051964	2.213007
274.781091	1496.765744	18.329715	-0.051895	2.207922
274.935521	1488.814857	18.334720	-0.051918	2.202857
274.902406	1480.876210	18.339725	-0.051907	2.197771
274.736921	1472.956916	18.344730	-0.051871	2.192673
274.753475	1464.974393	18.349735	-0.051869	2.187540
274.612279	1457.039459	18.354739	-0.051837	2.182411
274.775085	1449.082787	18.359744	-0.051862	2.177283
274.362249	1441.174763	18.364749	-0.051780	2.172122
274.396839	1433.218801	18.369754	-0.051782	2.166959
274.622917	1425.261428	18.374759	-0.051819	2.161800
274.523500	1417.328678	18.379763	-0.051795	2.156614
274.375873	1409.404784	18.384768	-0.051762	2.151418
274.424346	1401.434505	18.389773	-0.051766	2.146197
274.445545	1393.509298	18.394778	-0.051765	2.140990
274.300893	1385.596123	18.399783	-0.051733	2.135762
274.228069	1377.632844	18.404787	-0.051714	2.130496
274.468955	1369.666314	18.409792	-0.051753	2.125244
274.182379	1361.785362	18.414797	-0.051695	2.119986
273.833514	1353.916268	18.419802	-0.051625	2.114716
274.002272	1345.853707	18.424807	-0.051651	2.109354
273.939503	1337.906978	18.429811	-0.051634	2.104033
274.073583	1329.983971	18.434816	-0.051654	2.098734
274.019485	1322.052233	18.439821	-0.051639	2.093397
273.946135	1314.112073	18.444826	-0.051620	2.088039
273.975284	1306.191045	18.449831	-0.051620	2.082691
273.856802	1298.278664	18.454835	-0.051593	2.077319
273.882342	1290.348383	18.459840	-0.051592	2.071936
273.547712	1282.431693	18.464845	-0.051525	2.066512
273.439799	1274.515913	18.469850	-0.051500	2.061098
273.770279	1266.543197	18.474855	-0.051556	2.055674
273.647061	1258.599101	18.479859	-0.051528	2.050209
273.445426	1250.716303	18.484864	-0.051485	2.044764
273.469931	1242.774878	18.489869	-0.051484	2.039287
273.638483	1234.830858	18.494874	-0.051511	2.033809
273.601731	1226.876071	18.499879	-0.051499	2.028287
273.365004	1218.974454	18.504883	-0.051449	2.022766
273.216395	1211.091616	18.509888	-0.051416	2.017252
273.257642	1203.119669	18.514893	-0.051419	2.011681
272.961371	1195.231709	18.519898	-0.051359	2.006118
273.196934	1187.281697	18.524903	-0.051397	2.000551
272.993212	1179.403980	18.529907	-0.051354	1.994974
273.063433	1171.439841	18.534912	-0.051362	1.989348
272.879245	1163.527644	18.539917	-0.051323	1.983717
272.712596	1155.634327	18.544922	-0.051286	1.978085
272.768957	1147.692965	18.549927	-0.051292	1.972426
272.704808	1139.758761	18.554931	-0.051275	1.966743
272.900173	1131.826302	18.559936	-0.051306	1.961073
272.906373	1123.912644	18.564941	-0.051302	1.955379
272.578316	1115.989388	18.569946	-0.051235	1.949626
272.617110	1108.067206	18.574951	-0.051237	1.943897
272.603314	1100.133066	18.579955	-0.051230	1.938136
272.564449	1092.227768	18.584960	-0.051217	1.932376
272.578613	1084.291734	18.589965	-0.051215	1.926582
272.416159	1076.404901	18.594970	-0.051179	1.920787
272.306063	1068.521758	18.599975	-0.051154	1.914983
272.145119	1060.592642	18.604979	-0.051119	1.909122
272.270567	1052.665897	18.609984	-0.051137	1.903277
272.377923	1044.750973	18.614989	-0.051152	1.897420
272.116062	1036.866970	18.619994	-0.051098	1.891527
272.144830	1028.950171	18.624999	-0.051098	1.885623
272.034180	1021.060378	18.630003	-0.051072	1.879706
271.951905	1013.162726	18.635008	-0.051052	1.873767
271.964039	1005.207664	18.640013	-0.051049	1.867777
271.917804	997.312569	18.645018	-0.051035	1.861806
271.808496	989.436006	18.650023	-0.051009	1.855822
271.548969	981.529019	18.655027	-0.050956	1.849779
271.661851	973.622196	18.660032	-0.050972	1.843759
271.684623	965.719267	18.665037	-0.050971	1.837712
271.584046	957.818441	18.670042	-0.050947	1.831632
271.768781	949.884201	18.675047	-0.050976	1.825540
271.691268	941.995700	18.680051	-0.050956	1.819431
271.674579	934.116899	18.685056	-0.050948	1.813317
271.510226	926.226200	18.690061	-0.050912	1.807155
271.580417	918.323241	18.695066	-0.050920	1.800991
271.459530	910.461719	18.700071	-0.050893	1.794815
271.016176	902.545375	18.705075	-0.050805	1.788535
271.196167	894.626745	18.710080	-0.050833	1.782307
271.100419	886.753462	18.715085	-0.050810	1.776060
271.064570	878.847431	18.720090	-0.050798	1.769772
271.033653	870.976726	18.725095	-0.050787	1.763490
271.128941	863.074254	18.730099	-0.050800	1.757176
271.098492	855.189628	18.735104	-0.050789	1.750838
270.905257	847.317255	18.740109	-0.050748	1.744466
270.991396	839.431180	18.745114	-0.050759	1.738095
270.976639	831.554601	18.750119	-0.050751	1.731696
270.704476	823.687310	18.755123	-0.050695	1.725247
270.794198	815.825511	18.760128	-0.050707	1.718825
270.553267	807.964751	18.765133	-0.050657	1.712337
270.399672	800.076930	18.770138	-0.050623	1.705814
270.379062	792.210823	18.775143	-0.050614	1.699300
270.356093	784.314832	18.780147	-0.050605	1.692737
270.427551	776.424226	18.785152	-0.050613	1.686165
270.195797	768.591423	18.790157	-0.050564	1.679575
270.200423	760.715555	18.795162	-0.050560	1.672955
270.325151	752.807621	18.800167	-0.050578	1.666297
270.158784	744.968166	18.805171	-0.050542	1.659632
270.101296	737.121752	18.810176	-0.050526	1.652948
270.191806	729.214565	18.815181	-0.050538	1.646206
270.098004	721.391527	18.820186	-0.050515	1.639482
270.166881	713.504645	18.825191	-0.050523	1.632699
270.043783	705.608689	18.830195	-0.050495	1.625852
269.999252	697.780466	18.835200	-0.050482	1.619047
269.864942	689.936480	18.840205	-0.050451	1.612186
269.700895	682.093027	18.845210	-0.050416	1.605292
269.682957	674.264331	18.850215	-0.050407	1.598403
269.663493	666.392720	18.855219	-0.050398	1.591445
269.627598	658.552158	18.860224	-0.050387	1.584482
269.722979	650.690443	18.865229	-0.050399	1.577488
269.606548	642.858103	18.870234	-0.050372	1.570458
269.432565	635.053899	18.875239	-0.050335	1.563414
269.330506	627.217320	18.880243	-0.050311	1.556320
269.206335	619.380790	18.885248	-0.050283	1.549189
269.090415	611.552243	18.890253	-0.050256	1.542034
269.079715	603.713926	18.895258	-0.050249	1.534852
269.344527	595.835130	18.900263	-0.050293	1.527641
268.954373	588.063497	18.905267	-0.050215	1.520396
268.876552	580.263144	18.910272	-0.050196	1.513137
268.948503	572.388565	18.915277	-0.050204	1.505796
268.852347	564.594426	18.920282	-0.050181	1.498469
268.955755	556.759729	18.925287	-0.050195	1.491098
268.859305	548.952047	18.930291	-0.050172	1.483685
268.911474	541.145971	18.935296	-0.050176	1.476260
268.739100	533.301300	18.940301	-0.050139	1.468725
268.533563	525.522830	18.945306	-0.050096	1.461210
268.549800	517.720695	18.950311	-0.050094	1.453668
268.494512	509.904381	18.955315	-0.050078	1.446062
268.607585	502.107468	18.960320	-0.050094	1.438461
268.283093	494.348412	18.965325	-0.050029	1.430787
268.273560	486.543487	18.970330	-0.050022	1.423077
268.113757	478.789925	18.975335	-0.049987	1.415351
268.186977	470.964598	18.980339	-0.049996	1.407549
268.239867	463.191855	18.985344	-0.050000	1.399754
267.879612	455.455678	18.990349	-0.049928	1.391883
267.881890	447.652198	18.995354	-0.049924	1.383959
268.157264	439.839636	19.000359	-0.049970	1.376027
268.018545	432.080245	19.005363	-0.049939	1.368033
267.817118	424.355319	19.010368	-0.049896	1.360017
267.715743	416.599933	19.015373	-0.049872	1.351939
267.871113	408.799642	19.020378	-0.049896	1.343810
267.765402	401.078083	19.025383	-0.049871	1.335669
267.513698	393.346367	19.030387	-0.049819	1.327441
267.695884	385.586498	19.035392	-0.049848	1.319209
267.483996	377.796152	19.040397	-0.049804	1.310821
267.266604	370.036468	19.045402	-0.049758	1.302412
267.230839	362.323527	19.050407	-0.049747	1.294032
267.075870	354.603681	19.055411	-0.049713	1.285568
267.131785	346.894810	19.060416	-0.049718	1.277099
267.009355	339.181969	19.065421	-0.049690	1.268536
266.984816	331.472794	19.070426	-0.049681	1.259937
266.937325	323.779375	19.075431	-0.049667	1.251293
266.833967	316.081645	19.080435	-0.049642	1.242572
266.939199	308.384262	19.085440	-0.049657	1.233831
266.925436	300.672652	19.090445	-0.049649	1.224987
266.925417	292.994073	19.095450	-0.049644	1.216121
266.591354	285.364298	19.100455	-0.049577	1.207180
266.686787	277.674951	19.105459	-0.049590	1.198188
266.686560	270.010646	19.110464	-0.049585	1.189138
266.541368	262.371416	19.115469	-0.049553	1.180019
266.436503	254.730218	19.120474	-0.049528	1.170835
266.318504	247.113718	19.125479	-0.049501	1.161606
266.324224	239.457089	19.130483	-0.049497	1.152280
266.136264	231.828968	19.135488	-0.049457	1.142871
266.080378	224.205931	19.140493	-0.049442	1.133419
266.009393	216.593199	19.145498	-0.049424	1.123897
266.052803	208.984012	19.150503	-0.049427	1.114324
265.944327	201.386333	19.155507	-0.049402	1.104648
265.923665	193.811987	19.160512	-0.049393	1.094936
265.903521	186.224141	19.165517	-0.049384	1.085120
265.904691	178.662412	19.170522	-0.049379	1.075254
265.757429	171.113166	19.175527	-0.049347	1.065279
265.387528	163.618101	19.180531	-0.049273	1.055230
265.520236	156.042233	19.185536	-0.049293	1.045093
265.395970	148.539644	19.190541	-0.049265	1.034895
265.214392	141.034301	19.195546	-0.049226	1.024579
265.287149	133.521223	19.200551	-0.049235	1.014208
265.220399	126.022978	19.205555	-0.049217	1.003717
265.138459	118.553471	19.210560	-0.049197	0.993152
264.919806	111.086685	19.215565	-0.049152	0.982443
264.928464	103.623611	19.220570	-0.049148	0.971679
264.778743	96.208037	19.225575	-0.049116	0.960823
264.487249	88.818906	19.230579	-0.049057	0.949846
264.464094	81.403142	19.235584	-0.049047	0.938771
264.499316	73.992539	19.240589	-0.049049	0.927587
264.327602	66.647889	19.245594	-0.049012	0.916312
264.337205	59.498710	19.250599	-0.049009	0.905250