Fri Mar 12 12:06:59 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.646246	0.031928	0.000000	-0.000006	0.721076
0.486234	-0.042395	0.005005	0.000024	0.720874
0.530409	-0.051287	0.010010	0.000016	0.720872
0.750475	-0.086861	0.015014	-0.000025	0.720879
0.760646	-0.093585	0.020019	-0.000027	0.720869
0.853811	-0.105925	0.025024	-0.000044	0.720878
0.587427	-0.063123	0.030029	0.000005	0.720869
0.647866	-0.073325	0.035034	-0.000006	0.720870
0.750683	-0.086948	0.040038	-0.000025	0.720879
0.397700	-0.029280	0.045043	0.000041	0.720869
0.680164	-0.075093	0.050048	-0.000012	0.720878
0.647088	-0.072172	0.055053	-0.000006	0.720872
0.648641	-0.074465	0.060058	-0.000006	0.720868
0.504907	-0.043628	0.065062	0.000021	0.720878
0.550981	-0.056349	0.070067	0.000012	0.720869
0.818320	-0.165305	0.075072	-0.000038	0.720748
0.686825	-0.249893	0.080077	-0.000013	0.720536
0.533315	-0.223621	0.085082	0.000015	0.720534
0.660030	-0.243365	0.090086	-0.000008	0.720539
0.586745	-0.235582	0.095091	0.000006	0.720529
0.643713	-0.239259	0.100096	-0.000005	0.720542
0.706279	-0.253685	0.105101	-0.000017	0.720535
0.627006	-0.386578	0.110106	-0.000002	0.720246
0.581367	-0.388153	0.115110	0.000007	0.720226
0.606453	-0.397014	0.120115	0.000002	0.720218
0.754513	-0.418620	0.125120	-0.000026	0.720227
0.474196	-0.373529	0.130125	0.000027	0.720218
0.409408	-0.511153	0.135130	0.000039	0.719924
0.731047	-0.580271	0.140134	-0.000021	0.719900
0.538724	-0.549976	0.145139	0.000015	0.719893
0.558524	-0.549337	0.150144	0.000011	0.719901
0.549108	-0.644806	0.155149	0.000013	0.719709
0.636072	-0.717465	0.160154	-0.000003	0.719597
0.693527	-0.725475	0.165158	-0.000014	0.719601
0.512392	-0.697724	0.170163	0.000020	0.719592
0.583897	-0.859531	0.175168	0.000007	0.719298
0.548608	-0.868200	0.180173	0.000013	0.719269
0.530298	-0.866358	0.185178	0.000017	0.719266
0.706485	-0.981582	0.190182	-0.000016	0.719100
0.540426	-1.026220	0.195187	0.000015	0.718954
0.510686	-1.016527	0.200192	0.000020	0.718963
0.529903	-1.093397	0.205197	0.000017	0.718818
0.610429	-1.198095	0.210202	0.000002	0.718639
0.546691	-1.182902	0.215206	0.000014	0.718647
0.480909	-1.258596	0.220211	0.000026	0.718474
0.577651	-1.337722	0.225216	0.000008	0.718352
0.478124	-1.322994	0.230221	0.000027	0.718346
0.407874	-1.450485	0.235226	0.000040	0.718070
0.604150	-1.511671	0.240230	0.000003	0.718018
0.620666	-1.562724	0.245235	0.000000	0.717923
0.464100	-1.645774	0.250240	0.000029	0.717704
0.229587	-1.606091	0.255245	0.000073	0.717699
0.350286	-1.753926	0.260250	0.000051	0.717450
0.375043	-1.793185	0.265254	0.000046	0.717381
0.213696	-1.821038	0.270259	0.000076	0.717269
0.453734	-1.957388	0.275264	0.000032	0.717084
0.374321	-1.958782	0.280269	0.000046	0.717053
0.172337	-2.074425	0.285274	0.000084	0.716753
0.309800	-2.096105	0.290278	0.000059	0.716758
0.438728	-2.259001	0.295283	0.000035	0.716481
0.476517	-2.280904	0.300288	0.000028	0.716451
0.258650	-2.368449	0.305293	0.000068	0.716201
-0.094874	-2.343099	0.310298	0.000134	0.716127
-0.080065	-2.422912	0.315302	0.000131	0.715974
-0.458736	-2.405044	0.320307	0.000202	0.715876
-2.122342	-2.180047	0.325312	0.000511	0.715734
-3.089301	-2.104052	0.330317	0.000691	0.715543
-2.826091	-2.151486	0.335322	0.000643	0.715542
-3.010657	-2.160210	0.340326	0.000677	0.715460
-4.377850	-2.034082	0.345331	0.000931	0.715227
-3.687624	-2.156173	0.350336	0.000803	0.715228
-3.768282	-2.142231	0.355341	0.000818	0.715228
-4.306248	-2.172557	0.360346	0.000918	0.714977
-4.713055	-2.135281	0.365350	0.000994	0.714907
-5.043078	-2.079353	0.370355	0.001055	0.714902
-4.901097	-2.102674	0.375360	0.001029	0.714906
-5.334842	-2.143485	0.380365	0.001110	0.714671
-5.721228	-2.109909	0.385370	0.001182	0.714601
-5.288669	-2.183309	0.390374	0.001101	0.714609
-5.737074	-2.108411	0.395379	0.001185	0.714599
-6.024491	-2.148394	0.400384	0.001238	0.714418
-6.731395	-2.092909	0.405389	0.001370	0.714278
-6.749162	-2.091781	0.410394	0.001373	0.714274
-6.645334	-2.107012	0.415398	0.001354	0.714280
-6.788420	-2.086387	0.420403	0.001380	0.714270
-7.001859	-2.147793	0.425408	0.001420	0.714073
-7.894614	-2.040973	0.430413	0.001586	0.713969
-7.695188	-2.078815	0.435418	0.001549	0.713964
-7.179597	-2.166466	0.440422	0.001453	0.713973
-7.916546	-2.039209	0.445427	0.001590	0.713965
-7.673841	-2.111546	0.450432	0.001545	0.713907
-8.249712	-2.137182	0.455437	0.001653	0.713652
-8.523429	-2.092413	0.460442	0.001703	0.713644
-8.635964	-2.067254	0.465446	0.001724	0.713654
-8.373173	-2.117523	0.470451	0.001676	0.713647
-8.253198	-2.136224	0.475456	0.001653	0.713653
-8.921222	-2.084126	0.480461	0.001778	0.713519
-9.554654	-2.054659	0.485466	0.001896	0.713354
-8.896497	-2.168542	0.490470	0.001773	0.713360
-9.611184	-2.044379	0.495475	0.001906	0.713354
-9.781545	-2.011666	0.500480	0.001938	0.713359
-9.280735	-2.098810	0.505485	0.001845	0.713363
-9.523315	-2.099021	0.510490	0.001890	0.713276
-10.313532	-2.083949	0.515494	0.002037	0.713026
-10.213161	-2.106102	0.520499	0.002018	0.713018
-10.558971	-2.042089	0.525504	0.002083	0.713023
-10.264693	-2.094242	0.530509	0.002028	0.713023
-10.424083	-2.069367	0.535514	0.002057	0.713016
-10.246561	-2.095264	0.540518	0.002024	0.713027
-10.834845	-2.111223	0.545523	0.002134	0.712787
-11.377709	-2.053814	0.550528	0.002235	0.712709
-10.891045	-2.140090	0.555533	0.002144	0.712710
-11.160417	-2.095107	0.560538	0.002195	0.712704
-11.376910	-2.052254	0.565542	0.002235	0.712712
-11.506238	-2.032694	0.570547	0.002259	0.712705
-11.190531	-2.088077	0.575552	0.002200	0.712707
-11.912668	-2.121077	0.580557	0.002335	0.712385
-12.318552	-2.051963	0.585562	0.002410	0.712379
-12.022848	-2.100768	0.590566	0.002355	0.712386
-11.978711	-2.113015	0.595571	0.002347	0.712378
-12.238667	-2.064534	0.600576	0.002395	0.712382
-12.154203	-2.079775	0.605581	0.002380	0.712381
-12.347289	-2.058060	0.610586	0.002416	0.712356
-12.701955	-2.128486	0.615590	0.002482	0.712090
-13.018504	-2.076697	0.620595	0.002541	0.712081
-13.218488	-2.037689	0.625600	0.002578	0.712087
-13.044196	-2.067055	0.630605	0.002545	0.712091
-13.109164	-2.059899	0.635610	0.002558	0.712082
-12.931420	-2.086747	0.640614	0.002524	0.712092
-13.050202	-2.090878	0.645619	0.002547	0.712041
-13.776336	-2.103623	0.650624	0.002682	0.711758
-13.584846	-2.137426	0.655629	0.002646	0.711758
-14.153004	-2.039938	0.660634	0.002752	0.711751
-13.899962	-2.080911	0.665638	0.002705	0.711759
-13.922582	-2.079693	0.670643	0.002709	0.711754
-13.922388	-2.079096	0.675648	0.002709	0.711755
-13.896765	-2.117713	0.680653	0.002704	0.711687
-14.867478	-2.064730	0.685658	0.002885	0.711448
-14.247894	-2.169691	0.690662	0.002770	0.711458
-14.622207	-2.107877	0.695667	0.002839	0.711449
-14.987633	-2.042715	0.700672	0.002907	0.711449
-14.683207	-2.093904	0.705677	0.002851	0.711455
-14.936106	-2.051768	0.710682	0.002898	0.711449
-14.813488	-2.130582	0.715686	0.002875	0.711335
-15.887366	-2.040140	0.720691	0.003075	0.711134
-15.595342	-2.091195	0.725696	0.003021	0.711136
-15.742006	-2.064350	0.730701	0.003048	0.711137
-16.020997	-2.017327	0.735706	0.003100	0.711132
-15.479548	-2.109504	0.740710	0.002999	0.711141
-15.672586	-2.079050	0.745715	0.003035	0.711133
-15.912645	-2.057621	0.750720	0.003080	0.711090
-16.163832	-2.121875	0.755725	0.003127	0.710872
-16.342730	-2.093313	0.760730	0.003160	0.710866
-16.605761	-2.042017	0.765734	0.003209	0.710875
-16.496065	-2.065469	0.770739	0.003188	0.710867
-16.365756	-2.086729	0.775744	0.003164	0.710871
-16.340274	-2.088918	0.780749	0.003159	0.710875
-16.621612	-2.129903	0.785754	0.003212	0.710693
-17.424440	-2.065660	0.790758	0.003361	0.710536
-17.078791	-2.130650	0.795763	0.003297	0.710529
-17.466396	-2.061376	0.800768	0.003369	0.710530
-17.369194	-2.075370	0.805773	0.003351	0.710536
-17.254000	-2.098980	0.810778	0.003330	0.710530
-16.981120	-2.144164	0.815782	0.003279	0.710537
-17.795142	-2.140646	0.820787	0.003430	0.710254
-18.383613	-2.053503	0.825792	0.003540	0.710219
-18.409321	-2.046767	0.830797	0.003545	0.710223
-18.580079	-2.020471	0.835802	0.003576	0.710215
-18.200480	-2.085497	0.840806	0.003506	0.710220
-18.064908	-2.113284	0.845811	0.003481	0.710213
-18.350860	-2.061108	0.850816	0.003534	0.710215
-18.228999	-2.180689	0.855821	0.003511	0.710020
-19.210036	-2.072929	0.860826	0.003694	0.709885
-18.845103	-2.134680	0.865830	0.003626	0.709892
-19.118210	-2.089321	0.870835	0.003677	0.709885
-19.229758	-2.068967	0.875840	0.003697	0.709886
-18.815369	-2.139493	0.880845	0.003620	0.709893
-19.498135	-2.021362	0.885850	0.003747	0.709886
-19.443831	-2.151922	0.890854	0.003737	0.709644
-19.838344	-2.107247	0.895859	0.003811	0.709593
-20.015593	-2.075457	0.900864	0.003844	0.709593
-19.973364	-2.082158	0.905869	0.003836	0.709595
-20.202494	-2.044868	0.910874	0.003879	0.709588
-19.978519	-2.080330	0.915878	0.003837	0.709597
-19.974850	-2.084568	0.920883	0.003836	0.709590
-20.471475	-2.140061	0.925888	0.003929	0.709301
-20.813020	-2.097908	0.930893	0.003992	0.709264
-21.380158	-2.000531	0.935898	0.004098	0.709257
-21.109570	-2.043445	0.940902	0.004048	0.709267
-21.005867	-2.065861	0.945907	0.004028	0.709259
-21.017834	-2.062942	0.950912	0.004031	0.709261
-20.757298	-2.109097	0.955917	0.003982	0.709261
-20.951121	-2.155473	0.960922	0.004018	0.709099
-21.952886	-2.049180	0.965926	0.004205	0.708955
-21.750670	-2.087007	0.970931	0.004167	0.708951
-21.749094	-2.087204	0.975936	0.004167	0.708951
-21.623859	-2.105308	0.980941	0.004143	0.708960
-22.036063	-2.035385	0.985946	0.004220	0.708953
-22.095201	-2.021798	0.990950	0.004231	0.708959
-22.061812	-2.075110	0.995955	0.004225	0.708864
-23.098112	-2.005266	1.000960	0.004418	0.708634
-22.634634	-2.085060	1.005965	0.004332	0.708640
-23.055964	-2.013312	1.010970	0.004410	0.708633
-22.505832	-2.107069	1.015974	0.004308	0.708641
-23.025229	-2.017570	1.020979	0.004404	0.708635
-23.260915	-1.974818	1.025984	0.004448	0.708637
-22.418828	-2.122091	1.030989	0.004292	0.708642
-23.005624	-2.142179	1.035994	0.004401	0.708393
-23.606263	-2.055376	1.040998	0.004513	0.708352
-23.586778	-2.060167	1.046003	0.004509	0.708349
-23.706238	-2.038091	1.051008	0.004531	0.708351
-23.867382	-2.007884	1.056013	0.004561	0.708354
-23.710006	-2.040563	1.061018	0.004532	0.708345
-23.432428	-2.086369	1.066022	0.004480	0.708352
-24.300360	-2.072335	1.071027	0.004642	0.708070
-24.772650	-2.017272	1.076032	0.004730	0.708012
-24.252949	-2.107755	1.081037	0.004633	0.708016
-24.499676	-2.069068	1.086042	0.004679	0.708005
-24.865701	-1.999541	1.091046	0.004747	0.708014
-24.515722	-2.063861	1.096051	0.004682	0.708010
-24.537477	-2.060990	1.101056	0.004686	0.708008
-24.689717	-2.121475	1.106061	0.004714	0.707832
-26.011468	-1.956166	1.111066	0.004960	0.707691
-25.196961	-2.096903	1.116070	0.004809	0.707700
-25.516071	-2.041381	1.121075	0.004868	0.707698
-25.693182	-2.011558	1.126080	0.004901	0.707694
-25.349467	-2.069314	1.131085	0.004837	0.707701
-25.789564	-1.995379	1.136090	0.004919	0.707692
-25.628993	-2.038975	1.141094	0.004889	0.707662
-25.972951	-2.121218	1.146099	0.004953	0.707374
-26.458618	-2.035617	1.151104	0.005044	0.707372
-26.816746	-1.968276	1.156109	0.005110	0.707379
-26.386515	-2.050402	1.161114	0.005030	0.707368
-26.173152	-2.084265	1.166118	0.004991	0.707376
-26.426958	-2.041548	1.171123	0.005038	0.707371
-26.355955	-2.055287	1.176128	0.005025	0.707369
-26.393330	-2.191221	1.181133	0.005032	0.707083
-27.124008	-2.065911	1.186138	0.005168	0.707073
-27.413011	-2.010114	1.191142	0.005222	0.707082
-27.030204	-2.082270	1.196147	0.005150	0.707074
-26.960648	-2.097073	1.201152	0.005137	0.707069
-27.116962	-2.064811	1.206157	0.005166	0.707078
-27.456879	-2.065910	1.211162	0.005230	0.706954
-28.187719	-2.036605	1.216166	0.005366	0.706751
-27.875814	-2.094878	1.221171	0.005308	0.706746
-28.565347	-1.972700	1.226176	0.005436	0.706744
-28.136560	-2.045240	1.231181	0.005356	0.706752
-27.998692	-2.074162	1.236186	0.005331	0.706743
-28.278673	-2.020169	1.241190	0.005383	0.706751
-28.098321	-2.071546	1.246195	0.005349	0.706713
-28.755634	-2.092406	1.251200	0.005472	0.706436
-28.929103	-2.057788	1.256205	0.005504	0.706443
-29.385790	-1.978938	1.261210	0.005589	0.706438
-28.746948	-2.090169	1.266214	0.005470	0.706443
-28.987417	-2.047104	1.271219	0.005515	0.706443
-29.409087	-1.975467	1.276224	0.005593	0.706436
-28.866486	-2.068416	1.281229	0.005492	0.706444
-29.400539	-2.126604	1.286234	0.005592	0.706136
-30.033782	-2.016317	1.291238	0.005710	0.706130
-30.003693	-2.023927	1.296243	0.005704	0.706126
-29.783404	-2.064627	1.301248	0.005663	0.706123
-29.703563	-2.076407	1.306253	0.005648	0.706128
-30.020753	-2.024906	1.311258	0.005707	0.706118
-29.785726	-2.061089	1.316262	0.005664	0.706129
-30.314650	-2.099821	1.321267	0.005762	0.705862
-30.978559	-1.984453	1.326272	0.005886	0.705856
-30.530320	-2.058181	1.331277	0.005802	0.705868
-30.287236	-2.107679	1.336282	0.005757	0.705856
-30.603987	-2.049733	1.341286	0.005816	0.705859
-30.643007	-2.043121	1.346291	0.005823	0.705858
-30.499836	-2.134179	1.351296	0.005797	0.705726
-31.601768	-2.038526	1.356301	0.006002	0.705523
-31.606490	-2.040704	1.361306	0.006003	0.705517
-31.260096	-2.099501	1.366310	0.005938	0.705523
-31.373644	-2.079641	1.371315	0.005959	0.705522
-31.787831	-2.007506	1.376320	0.006036	0.705519
-31.374896	-2.077661	1.381325	0.005960	0.705526
-31.385729	-2.180673	1.386330	0.005962	0.705315
-32.708659	-1.997638	1.391334	0.006208	0.705208
-32.744261	-1.991751	1.396339	0.006214	0.705208
-32.262199	-2.081405	1.401344	0.006125	0.705200
-32.370648	-2.056870	1.406349	0.006145	0.705211
-32.927101	-1.961503	1.411354	0.006249	0.705203
-32.576538	-2.019457	1.416358	0.006183	0.705212
-32.179282	-2.156370	1.421363	0.006109	0.705079
-33.484323	-2.021650	1.426368	0.006352	0.704882
-32.815598	-2.136871	1.431373	0.006228	0.704890
-33.206430	-2.073583	1.436378	0.006301	0.704877
-33.154766	-2.076859	1.441382	0.006291	0.704889
-33.257316	-2.060973	1.446387	0.006310	0.704884
-33.348563	-2.046522	1.451392	0.006327	0.704880
-33.393464	-2.154361	1.456397	0.006336	0.704647
-34.345793	-2.018741	1.461402	0.006513	0.704578
-34.193109	-2.040378	1.466406	0.006484	0.704589
-33.706621	-2.128807	1.471411	0.006394	0.704586
-34.356811	-2.013816	1.476416	0.006515	0.704584
-34.173506	-2.043468	1.481421	0.006481	0.704590
-34.181297	-2.045327	1.486426	0.006482	0.704583
-34.692370	-2.099858	1.491430	0.006577	0.704290
-35.418353	-1.985677	1.496435	0.006712	0.704259
-35.187920	-2.029580	1.501440	0.006670	0.704253
-34.869275	-2.082318	1.506445	0.006610	0.704262
-35.445049	-1.982255	1.511450	0.006717	0.704256
-35.126683	-2.036879	1.516454	0.006658	0.704261
-34.817086	-2.091527	1.521459	0.006601	0.704262
-35.413573	-2.075685	1.526464	0.006712	0.704079
-36.265522	-1.984474	1.531469	0.006870	0.703957
-35.757132	-2.079674	1.536474	0.006776	0.703948
-35.696544	-2.089348	1.541478	0.006764	0.703950
-36.002541	-2.034168	1.546483	0.006821	0.703951
-36.006469	-2.035590	1.551488	0.006822	0.703947
-35.636276	-2.096709	1.556493	0.006753	0.703957
-36.269903	-2.093777	1.561498	0.006871	0.703735
-36.901897	-2.029912	1.566502	0.006989	0.703636
-36.428318	-2.114496	1.571507	0.006901	0.703636
-37.012384	-2.014572	1.576512	0.007009	0.703628
-37.190774	-1.978274	1.581517	0.007043	0.703637
-36.882698	-2.037296	1.586522	0.006985	0.703628
-36.511077	-2.101342	1.591526	0.006916	0.703633
-36.967952	-2.104579	1.596531	0.007001	0.703462
-37.869026	-2.006016	1.601536	0.007169	0.703336
-37.069035	-2.144237	1.606541	0.007020	0.703345
-37.579744	-2.056732	1.611546	0.007115	0.703338
-37.734475	-2.028597	1.616550	0.007144	0.703339
-37.367662	-2.094379	1.621555	0.007076	0.703338
-37.818781	-2.017614	1.626560	0.007160	0.703331
-38.222845	-2.094384	1.631565	0.007235	0.703031
-38.471000	-2.067794	1.636570	0.007281	0.702995
-38.527482	-2.054432	1.641574	0.007292	0.703002
-38.600625	-2.041192	1.646579	0.007305	0.703002
-38.625543	-2.038637	1.651584	0.007310	0.702998
-38.378394	-2.077210	1.656589	0.007264	0.703009
-38.570408	-2.048379	1.661594	0.007300	0.702998
-39.064061	-2.098517	1.666598	0.007392	0.702719
-39.385504	-2.055875	1.671603	0.007451	0.702689
-39.647379	-2.012962	1.676608	0.007500	0.702682
-39.296639	-2.068387	1.681613	0.007435	0.702696
-39.421689	-2.051878	1.686618	0.007458	0.702685
-39.119381	-2.102144	1.691622	0.007402	0.702692
-39.467943	-2.040684	1.696627	0.007467	0.702690
-39.986353	-2.098543	1.701632	0.007563	0.702387
-39.903581	-2.118778	1.706637	0.007548	0.702376
-40.392063	-2.038082	1.711642	0.007639	0.702363
-40.395555	-2.034172	1.716646	0.007640	0.702369
-40.355814	-2.042294	1.721651	0.007632	0.702367
-40.430169	-2.030922	1.726656	0.007646	0.702363
-40.289161	-2.052044	1.731661	0.007620	0.702371
-40.706072	-2.110099	1.736666	0.007697	0.702104
-41.176436	-2.042045	1.741670	0.007785	0.702072
-41.188891	-2.038120	1.746675	0.007787	0.702075
-41.261234	-2.029151	1.751680	0.007801	0.702067
-40.994986	-2.070523	1.756685	0.007751	0.702080
-41.194158	-2.041872	1.761690	0.007788	0.702066
-41.413955	-2.000088	1.766694	0.007829	0.702071
-41.420736	-2.127587	1.771699	0.007831	0.701810
-42.214902	-2.020378	1.776704	0.007978	0.701741
-42.082974	-2.040040	1.781709	0.007954	0.701749
-41.942680	-2.068869	1.786714	0.007928	0.701741
-41.871087	-2.080780	1.791718	0.007914	0.701743
-41.716522	-2.107449	1.796723	0.007886	0.701744
-42.260529	-2.014373	1.801728	0.007987	0.701737
-42.426618	-2.127319	1.806733	0.008018	0.701448
-42.598391	-2.104818	1.811738	0.008050	0.701431
-43.033006	-2.024305	1.816742	0.008131	0.701438
-42.700752	-2.083392	1.821747	0.008069	0.701438
-42.761420	-2.076346	1.826752	0.008080	0.701430
-42.862177	-2.054325	1.831757	0.008099	0.701438
-43.088899	-2.049397	1.836762	0.008141	0.701367
-43.775433	-2.048533	1.841766	0.008269	0.701120
-43.722353	-2.056721	1.846771	0.008259	0.701123
-44.172844	-1.979003	1.851776	0.008343	0.701118
-43.774749	-2.045902	1.856781	0.008269	0.701126
-43.822093	-2.041076	1.861786	0.008278	0.701119
-44.029960	-2.003193	1.866790	0.008316	0.701120
-43.948187	-2.016768	1.871795	0.008301	0.701122
-43.970180	-2.110553	1.876800	0.008305	0.700924
-44.417245	-2.053476	1.881805	0.008389	0.700878
-44.499013	-2.041393	1.886810	0.008404	0.700873
-44.305362	-2.075073	1.891814	0.008368	0.700875
-44.252718	-2.084262	1.896819	0.008358	0.700875
-44.628223	-2.019336	1.901824	0.008428	0.700871
-44.435392	-2.127439	1.906829	0.008392	0.700722
-45.330736	-2.061265	1.911834	0.008559	0.700532
-45.181167	-2.086353	1.916838	0.008531	0.700536
-45.197982	-2.082233	1.921843	0.008534	0.700538
-45.754478	-1.989455	1.926848	0.008638	0.700525
-45.214429	-2.080173	1.931853	0.008537	0.700536
-45.653232	-2.005227	1.936858	0.008619	0.700529
-45.866342	-2.080278	1.941862	0.008659	0.700300
-46.232862	-2.052742	1.946867	0.008727	0.700223
-46.611731	-1.990675	1.951872	0.008797	0.700212
-46.242641	-2.051064	1.956877	0.008729	0.700223
-46.276529	-2.049171	1.961882	0.008735	0.700215
-46.375917	-2.030941	1.966886	0.008753	0.700216
-46.274594	-2.048234	1.971891	0.008735	0.700217
-46.504783	-2.118301	1.976896	0.008777	0.699992
-47.305470	-2.022858	1.981901	0.008926	0.699896
-47.214836	-2.041862	1.986906	0.008910	0.699890
-46.954232	-2.087678	1.991910	0.008861	0.699891
-46.928981	-2.090368	1.996915	0.008856	0.699895
-47.153465	-2.051260	2.001920	0.008898	0.699893
-47.579475	-2.087988	2.011917	0.008978	0.699665
-47.940542	-2.056616	2.021914	0.009045	0.699597
-47.956214	-2.053694	2.031910	0.009048	0.699598
-47.925836	-2.060140	2.041907	0.009042	0.699596
-47.800252	-2.082525	2.051904	0.009019	0.699596
-47.955895	-2.055564	2.061901	0.009048	0.699594
-47.988122	-2.048227	2.071898	0.009054	0.699597
-47.944017	-2.054888	2.081894	0.009046	0.699600
-47.865348	-2.069830	2.091891	0.009031	0.699598
-47.907991	-2.011085	2.101888	0.009039	0.699701
-47.069756	-2.064444	2.111885	0.008883	0.699897
-47.157130	-2.048966	2.121882	0.008899	0.699896
-47.168965	-2.046112	2.131878	0.008901	0.699898
-47.182491	-2.045383	2.141875	0.008904	0.699894
-47.249254	-2.033619	2.151872	0.008916	0.699894
-47.203085	-2.004211	2.161869	0.008908	0.699970
-46.315530	-2.041780	2.171866	0.008742	0.700215
-46.209057	-2.060139	2.181862	0.008723	0.700216
-46.305882	-2.042552	2.191859	0.008741	0.700217
-46.309602	-2.042455	2.201856	0.008741	0.700216
-45.518183	-2.060520	2.211853	0.008594	0.700465
-45.606085	-2.012220	2.221850	0.008610	0.700532
-45.202987	-2.083476	2.231846	0.008535	0.700533
-45.468888	-2.034735	2.241843	0.008585	0.700535
-45.038418	-1.998938	2.251840	0.008505	0.700764
-44.671915	-2.011639	2.261837	0.008436	0.700870
-44.502594	-2.041976	2.271834	0.008405	0.700870
-44.175309	-2.099402	2.281830	0.008344	0.700872
-43.865921	-2.061129	2.291827	0.008286	0.701061
-43.731509	-2.055763	2.301824	0.008261	0.701121
-43.589663	-2.083052	2.311821	0.008235	0.701116
-43.836483	-2.018538	2.321818	0.008281	0.701158
-42.839830	-2.058811	2.331814	0.008095	0.701436
-42.620294	-2.098680	2.341811	0.008055	0.701435
-42.790997	-2.066570	2.351808	0.008086	0.701438
-42.579014	-2.032123	2.361805	0.008047	0.701584
-42.035388	-2.052125	2.371802	0.007946	0.701740
-42.031363	-2.051749	2.381798	0.007945	0.701742
-42.050636	-2.021381	2.391795	0.007949	0.701797
-41.203412	-2.037615	2.401792	0.007791	0.702069
-41.140128	-2.048849	2.411789	0.007779	0.702070
-41.238792	-2.029699	2.421786	0.007797	0.702073
-40.592326	-2.038642	2.431782	0.007677	0.702288
-40.519326	-2.011872	2.441779	0.007663	0.702368
-40.305603	-2.050007	2.451776	0.007624	0.702368
-40.175983	-2.010516	2.461773	0.007600	0.702494
-39.316685	-2.065499	2.471770	0.007440	0.702693
-39.171033	-2.091651	2.481766	0.007413	0.702693
-39.384106	-2.053261	2.491763	0.007452	0.702693
-38.827833	-2.035535	2.501760	0.007349	0.702930
-38.620708	-2.036393	2.511757	0.007310	0.703002
-38.470751	-2.061455	2.521754	0.007282	0.703006
-38.421809	-2.022573	2.531750	0.007273	0.703102
-37.480300	-2.071871	2.541747	0.007098	0.703341
-37.487215	-2.071169	2.551744	0.007099	0.703340
-37.693785	-2.033785	2.561741	0.007137	0.703341
-37.207551	-2.019100	2.571738	0.007047	0.703546
-36.850754	-2.039134	2.581734	0.006981	0.703634
-36.992565	-2.013722	2.591731	0.007007	0.703634
-36.609491	-2.027241	2.601728	0.006936	0.703744
-35.989186	-2.036822	2.611725	0.006820	0.703948
-35.953683	-2.042171	2.621722	0.006814	0.703950
-36.058936	-2.022503	2.631718	0.006833	0.703952
-35.310734	-2.003105	2.641715	0.006694	0.704260
-35.126599	-2.037123	2.651712	0.006660	0.704258
-35.064557	-2.049646	2.661709	0.006648	0.704255
-34.737303	-2.013841	2.671706	0.006587	0.704444
-34.166572	-2.045232	2.681702	0.006481	0.704586
-34.352597	-2.011280	2.691699	0.006516	0.704588
-33.884974	-2.092076	2.701696	0.006429	0.704593
-33.542167	-2.008789	2.711693	0.006365	0.704884
-33.122855	-2.083647	2.721690	0.006287	0.704884
-33.383079	-2.036739	2.731686	0.006335	0.704885
-33.143053	-1.989525	2.741683	0.006290	0.705066
-32.447159	-2.041878	2.751680	0.006161	0.705210
-32.640692	-2.009034	2.761677	0.006197	0.705207
-32.448606	-2.015858	2.771674	0.006161	0.705262
-31.602083	-2.036981	2.781670	0.006003	0.705523
-31.437199	-2.065470	2.791667	0.005973	0.705525
-31.513166	-2.052809	2.801664	0.005987	0.705523
-31.346654	-1.980397	2.811661	0.005956	0.705728
-30.581835	-2.050751	2.821658	0.005814	0.705861
-30.842303	-2.003647	2.831654	0.005862	0.705863
-30.715676	-2.000677	2.841651	0.005838	0.705914
-30.060110	-2.012781	2.851648	0.005716	0.706124
-29.628617	-2.090348	2.861645	0.005636	0.706123
-29.680685	-2.079966	2.871642	0.005646	0.706125
-29.353076	-2.035984	2.881638	0.005585	0.706331
-28.788129	-2.081378	2.891635	0.005480	0.706442
-29.021763	-2.039642	2.901632	0.005523	0.706442
-29.147751	-1.993253	2.911629	0.005547	0.706490
-28.084505	-2.054004	2.921626	0.005349	0.706749
-28.242078	-2.024854	2.931622	0.005378	0.706751
-27.876268	-2.088765	2.941619	0.005310	0.706754
-27.755657	-1.996344	2.951616	0.005287	0.706983
-27.150534	-2.057251	2.961613	0.005175	0.707077
-27.178560	-2.051738	2.971610	0.005180	0.707078
-27.247464	-2.004368	2.981606	0.005193	0.707148
-26.324721	-2.055480	2.991603	0.005021	0.707376
-26.334302	-2.053021	3.001600	0.005023	0.707377
-26.375652	-2.048131	3.011597	0.005031	0.707372
-25.825977	-2.025616	3.021594	0.004928	0.707614
-25.651816	-2.014763	3.031590	0.004896	0.707698
-25.457759	-2.048990	3.041587	0.004860	0.707699
-25.523560	-1.982072	3.051584	0.004872	0.707809
-24.409222	-2.080274	3.061581	0.004665	0.708011
-24.539946	-2.057860	3.071578	0.004689	0.708009
-24.505419	-2.062443	3.081574	0.004682	0.708012
-23.922814	-2.046301	3.091571	0.004574	0.708252
-23.879282	-2.005495	3.101568	0.004566	0.708350
-23.760942	-2.026732	3.111565	0.004544	0.708349
-23.730714	-1.989125	3.121562	0.004538	0.708436
-22.808394	-2.052534	3.131558	0.004367	0.708638
-22.701597	-2.071518	3.141555	0.004347	0.708638
-23.246601	-1.975229	3.151552	0.004448	0.708636
-22.470178	-1.970527	3.161549	0.004304	0.708923
-22.336781	-1.979535	3.171546	0.004279	0.708952
-21.864623	-2.063401	3.181542	0.004191	0.708953
-21.563464	-2.021527	3.191539	0.004135	0.709144
-21.385493	-1.993954	3.201536	0.004102	0.709263
-21.170354	-2.032129	3.211533	0.004062	0.709263
-21.040794	-2.036226	3.221530	0.004038	0.709301
-20.312011	-2.019564	3.231526	0.003902	0.709594
-20.175535	-2.042742	3.241523	0.003876	0.709596
-20.233538	-2.033370	3.251520	0.003887	0.709594
-20.066457	-1.987558	3.261517	0.003856	0.709745
-19.412434	-2.031012	3.271514	0.003734	0.709892
-19.493342	-2.015604	3.281510	0.003749	0.709894
-19.306722	-2.042909	3.291507	0.003715	0.709905
-18.797578	-1.978638	3.301504	0.003620	0.710215
-18.328788	-2.063226	3.311501	0.003533	0.710213
-18.687432	-1.999105	3.321498	0.003599	0.710214
-17.995680	-2.033501	3.331494	0.003471	0.710391
-17.488772	-2.052540	3.341491	0.003376	0.710533
-17.591173	-2.036354	3.351488	0.003395	0.710529
-17.706617	-2.016670	3.361485	0.003417	0.710528
-16.848417	-2.001342	3.371482	0.003257	0.710863
-16.532594	-2.053461	3.381478	0.003198	0.710872
-16.705832	-2.022891	3.391475	0.003231	0.710871
-16.717252	-1.976527	3.401472	0.003233	0.710960
-15.937354	-2.026371	3.411469	0.003087	0.711137
-16.015581	-2.012145	3.421466	0.003102	0.711138
-15.933661	-2.020583	3.431462	0.003087	0.711150
-15.354070	-1.970454	3.441459	0.002979	0.711456
-14.973075	-2.038647	3.451456	0.002908	0.711456
-15.153223	-2.008924	3.461453	0.002942	0.711451
-14.689143	-1.988430	3.471450	0.002855	0.711657
-14.270881	-2.010192	3.481446	0.002777	0.711762
-14.434439	-1.981663	3.491443	0.002808	0.711761
-14.080977	-1.987439	3.501440	0.002742	0.711875
-13.351192	-2.010498	3.511437	0.002606	0.712088
-13.622492	-1.961988	3.521434	0.002657	0.712088
-13.202343	-2.036174	3.531430	0.002578	0.712090
-13.003938	-1.930853	3.541427	0.002541	0.712370
-12.453345	-2.022160	3.551424	0.002439	0.712383
-12.792780	-1.961863	3.561421	0.002502	0.712383
-12.024073	-1.988750	3.571418	0.002359	0.712602
-11.272337	-2.068439	3.581414	0.002219	0.712710
-11.419629	-2.042889	3.591411	0.002246	0.712709
-11.295795	-2.066159	3.601408	0.002223	0.712706
-10.672816	-2.052770	3.611405	0.002107	0.712954
-10.588874	-2.036221	3.621402	0.002092	0.713017
-10.370285	-2.074332	3.631398	0.002051	0.713018
-10.406018	-2.067168	3.641395	0.002058	0.713020
-9.553961	-2.072298	3.651392	0.001899	0.713312
-9.703544	-2.024851	3.661389	0.001927	0.713353
-9.490819	-2.060934	3.671386	0.001887	0.713356
-9.646400	-2.012063	3.681382	0.001916	0.713399
-8.808067	-2.035301	3.691379	0.001760	0.713649
-8.596721	-2.073533	3.701376	0.001721	0.713648
-8.588646	-2.075904	3.711373	0.001720	0.713646
-8.508366	-2.024821	3.721370	0.001705	0.713776
-7.551273	-2.098599	3.731366	0.001526	0.713968
-7.839620	-2.047805	3.741363	0.001580	0.713967
-7.828733	-2.050991	3.751360	0.001578	0.713965
-7.124558	-2.041876	3.761357	0.001447	0.714232
-6.641616	-2.108823	3.771354	0.001357	0.714270
-6.814815	-2.074925	3.781350	0.001389	0.714276
-6.826917	-2.049544	3.791347	0.001392	0.714322
-5.810961	-2.088735	3.801344	0.001202	0.714604
-5.769739	-2.097091	3.811341	0.001195	0.714602
-5.833132	-2.086495	3.821338	0.001207	0.714600
-5.784675	-2.035161	3.831334	0.001198	0.714719
-4.651004	-2.143205	3.841331	0.000987	0.714906
-4.888130	-2.102958	3.851328	0.001031	0.714902
-5.065455	-2.070647	3.861325	0.001064	0.714903
-4.344467	-2.111486	3.871322	0.000929	0.715077
-3.795576	-2.132437	3.881318	0.000827	0.715229
-4.099604	-2.079092	3.891315	0.000884	0.715228
-3.994510	-2.097881	3.901312	0.000864	0.715228
-3.375509	-2.077508	3.911309	0.000749	0.715487
-3.016760	-2.114406	3.921306	0.000682	0.715540
-3.132121	-2.091754	3.931302	0.000704	0.715544
-2.977568	-2.098344	3.941299	0.000675	0.715586
-2.351988	-2.063258	3.951296	0.000559	0.715876
-2.394422	-2.055727	3.961293	0.000566	0.715876
-2.213756	-2.085690	3.971290	0.000533	0.715880
-2.230408	-1.994718	3.981286	0.000536	0.716055
-1.725987	-2.047756	3.991283	0.000442	0.716128
-1.671160	-2.058221	4.001280	0.000432	0.716126
-1.529216	-1.980631	4.011277	0.000405	0.716330
-1.270032	-1.969761	4.021274	0.000357	0.716443
-1.243992	-1.973678	4.031270	0.000352	0.716444
-1.145171	-1.858432	4.041267	0.000334	0.716707
-1.020200	-1.858806	4.051264	0.000311	0.716751
-1.008514	-1.793349	4.061261	0.000308	0.716884
-1.029766	-1.689896	4.071258	0.000312	0.717081
-0.980767	-1.652627	4.081254	0.000303	0.717172
-0.904658	-1.562485	4.091251	0.000289	0.717378
-0.785523	-1.517292	4.101248	0.000267	0.717509
-0.866034	-1.407349	4.111245	0.000282	0.717698
-0.913986	-1.288191	4.121242	0.000290	0.717916
-0.625606	-1.276495	4.131238	0.000237	0.718041
-0.600576	-1.126041	4.141235	0.000232	0.718347
-0.529863	-1.056023	4.151232	0.000219	0.718510
-0.577122	-0.960936	4.161229	0.000228	0.718681
-0.357989	-0.858657	4.171226	0.000187	0.718960
-0.213980	-0.770758	4.181222	0.000160	0.719184
-0.234853	-0.662058	4.191219	0.000164	0.719391
-0.204812	-0.548639	4.201216	0.000158	0.719625
-0.260535	-0.400872	4.211213	0.000168	0.719897
-0.155438	-0.272924	4.221210	0.000149	0.720186
-0.084885	-0.150632	4.231206	0.000136	0.720451
-0.110561	-0.000076	4.241203	0.000140	0.720739
0.000000	0.127864	4.251200	0.000120	0.721029
0.127478	0.734988	4.256205	0.000095	0.722267
0.078610	2.015145	4.261210	0.000104	0.724760
0.488019	3.801099	4.266214	0.000026	0.728389
0.982889	6.138214	4.271219	-0.000067	0.733097
1.197687	9.019673	4.276224	-0.000109	0.738725
1.344003	12.404246	4.281229	-0.000139	0.745245
1.756757	16.186122	4.286234	-0.000218	0.752547
2.051292	20.394591	4.291238	-0.000276	0.760536
2.260339	25.021025	4.296243	-0.000318	0.769184
2.758049	29.951713	4.301248	-0.000413	0.778385
3.438547	35.210112	4.306253	-0.000544	0.788126
3.869117	40.828547	4.311258	-0.000627	0.798309
4.186397	46.764584	4.316262	-0.000690	0.808886
4.655736	52.964373	4.321267	-0.000782	0.819829
5.017228	59.447164	4.326272	-0.000853	0.831078
5.599787	66.117597	4.331277	-0.000966	0.842558
6.092678	73.026644	4.336282	-0.001062	0.854253
6.679498	80.126048	4.341286	-0.001176	0.866130
7.162882	87.435895	4.346291	-0.001271	0.878155
11.057051	94.324055	4.351296	-0.002001	0.890301
13.917417	101.640877	4.356301	-0.002538	0.902670
14.142712	109.571835	4.361306	-0.002585	0.915106
14.519057	117.566082	4.366310	-0.002660	0.927512
15.683356	125.553851	4.371315	-0.002882	0.939952
16.857769	133.648626	4.376320	-0.003106	0.952391
17.536996	141.915399	4.381325	-0.003238	0.964794
19.010063	150.142310	4.386330	-0.003518	0.977183
19.987061	158.531478	4.391334	-0.003705	0.989524
20.884755	166.977813	4.396339	-0.003878	1.001774
21.742785	175.454322	4.401344	-0.004043	1.013908
22.454022	184.007491	4.406349	-0.004181	1.025969
23.369706	192.553792	4.411354	-0.004357	1.037928
24.449768	201.102806	4.416358	-0.004564	1.049793
25.181190	209.749918	4.421363	-0.004706	1.061575
25.768173	218.430810	4.426368	-0.004821	1.073239
26.801807	227.035439	4.431373	-0.005019	1.084778
28.005219	235.624255	4.436378	-0.005248	1.096212
29.050925	244.243502	4.441382	-0.005449	1.107532
29.555801	252.974537	4.446387	-0.005548	1.118761
30.822355	261.551893	4.451392	-0.005790	1.129849
31.869880	270.197170	4.456397	-0.005990	1.140866
32.461136	278.927952	4.461402	-0.006106	1.151787
32.704742	287.664750	4.466406	-0.006157	1.162539
33.641226	296.271017	4.471411	-0.006337	1.173178
34.411367	304.875827	4.476416	-0.006486	1.183685
34.987045	313.529923	4.481421	-0.006599	1.194119
35.247224	322.192786	4.486426	-0.006653	1.204409
36.003691	330.769005	4.491430	-0.006800	1.214609
36.698000	339.338391	4.496435	-0.006934	1.224703
37.345322	347.922802	4.501440	-0.007061	1.234723
38.158714	356.439989	4.506445	-0.007218	1.244617
38.957744	364.962571	4.511450	-0.007372	1.254436
39.363674	373.518349	4.516454	-0.007453	1.264142
40.132242	382.028662	4.521459	-0.007602	1.273790
40.839781	390.495261	4.526464	-0.007739	1.283306
41.686281	398.959106	4.531469	-0.007902	1.292775
42.404817	407.431128	4.536474	-0.008041	1.302159
42.978687	415.990911	4.541478	-0.008154	1.311545
43.645824	424.484557	4.546483	-0.008284	1.320810
44.331298	432.885372	4.551488	-0.008417	1.329914
44.955572	441.313614	4.556493	-0.008538	1.338974
45.350147	449.757120	4.561498	-0.008617	1.347948
46.090537	458.131555	4.566502	-0.008761	1.356851
46.897621	466.478913	4.571507	-0.008916	1.365680
47.722754	474.822889	4.576512	-0.009075	1.374450
48.451696	483.182791	4.581517	-0.009217	1.383165
48.940613	491.595974	4.586522	-0.009313	1.391839
49.492886	499.955522	4.591526	-0.009421	1.400415
50.021980	508.319364	4.596531	-0.009525	1.408939
50.089696	516.740290	4.601536	-0.009543	1.417392
50.760091	525.040642	4.606541	-0.009674	1.425774
51.589498	533.340300	4.611546	-0.009833	1.434133
52.251583	541.632798	4.616550	-0.009962	1.442408
52.999036	549.926775	4.621555	-0.010107	1.450651
53.640598	558.226640	4.626560	-0.010232	1.458836
54.166071	566.546412	4.631565	-0.010335	1.466976
55.108565	574.845931	4.636570	-0.010516	1.475117
55.819011	583.103967	4.641574	-0.010653	1.483137
56.140293	591.435222	4.646579	-0.010719	1.491122
56.516855	599.739169	4.651584	-0.010794	1.499048
57.199302	607.993202	4.656589	-0.010927	1.506932
57.702959	616.288491	4.661594	-0.011026	1.514786
57.881318	624.589213	4.666598	-0.011064	1.522555
58.529321	632.835867	4.671603	-0.011190	1.530305
58.725776	641.142587	4.676608	-0.011232	1.538003
59.362948	649.350262	4.681613	-0.011356	1.545638
60.159876	657.570401	4.686618	-0.011510	1.553270
60.553216	665.816953	4.691622	-0.011589	1.560829
60.937871	674.066183	4.696627	-0.011666	1.568353
61.321803	682.314152	4.701632	-0.011743	1.575839
62.086622	690.497888	4.706637	-0.011890	1.583288
62.673373	698.724005	4.711642	-0.012005	1.590713
63.004925	706.971851	4.716646	-0.012072	1.598087
63.477889	715.182436	4.721651	-0.012165	1.605413
63.651659	723.452624	4.726656	-0.012203	1.612717
64.022324	731.675629	4.731661	-0.012278	1.619974
64.566804	739.860641	4.736666	-0.012384	1.627189
65.055207	748.126016	4.741670	-0.012481	1.634434
65.852796	756.258629	4.746675	-0.012634	1.641575
66.281973	764.439048	4.751680	-0.012720	1.648676
66.879826	772.623839	4.756685	-0.012836	1.655772
67.258453	780.823390	4.761690	-0.012912	1.662821
67.584321	789.030674	4.766694	-0.012978	1.669840
68.168532	797.230441	4.771699	-0.013092	1.676857
68.306943	805.441908	4.776704	-0.013123	1.683796
68.705454	813.626352	4.781709	-0.013203	1.690717
69.119882	821.814401	4.786714	-0.013285	1.697616
69.815958	829.945193	4.791718	-0.013420	1.704475
70.240712	838.158300	4.796723	-0.013505	1.711340
70.501241	846.345096	4.801728	-0.013559	1.718134
71.139444	854.478239	4.806733	-0.013683	1.724906
71.664731	862.643243	4.811738	-0.013786	1.731663
72.662595	870.717361	4.816742	-0.013977	1.738380
73.600587	878.825622	4.821747	-0.014157	1.745090
73.856455	887.049189	4.826752	-0.014210	1.751782
74.102291	895.268644	4.831757	-0.014261	1.758443
74.412198	903.427431	4.836762	-0.014324	1.765039
75.144611	911.552816	4.841766	-0.014466	1.771635
75.681316	919.728518	4.846771	-0.014571	1.778223
75.907895	927.911070	4.851776	-0.014618	1.784754
76.320709	936.114697	4.856781	-0.014701	1.791300
77.023122	944.246195	4.861786	-0.014837	1.797801
77.653451	952.340409	4.866790	-0.014959	1.804240
77.885628	960.532716	4.871795	-0.015008	1.810685
78.230942	968.676485	4.876800	-0.015078	1.817082
79.100719	976.749335	4.881805	-0.015245	1.823465
79.280251	984.945313	4.886810	-0.015283	1.829838
79.697140	993.088811	4.891814	-0.015366	1.836176
80.602103	1001.172483	4.896819	-0.015540	1.842505
81.180146	1009.298681	4.901824	-0.015653	1.848805
81.489254	1017.476160	4.906829	-0.015716	1.855092
82.110599	1025.592041	4.911834	-0.015837	1.861347
82.485277	1033.740766	4.916838	-0.015912	1.867577
82.808652	1041.947633	4.921843	-0.015978	1.873824
83.347018	1050.032505	4.926848	-0.016083	1.879983
83.988394	1058.132673	4.931853	-0.016208	1.886145
84.328376	1066.287804	4.936858	-0.016276	1.892293
84.424403	1074.464329	4.941862	-0.016300	1.898410
84.890604	1082.574031	4.946867	-0.016392	1.904500
85.247730	1090.707679	4.951872	-0.016463	1.910575
85.555739	1098.856383	4.956877	-0.016526	1.916637
85.939907	1106.954788	4.961882	-0.016603	1.922650
86.406217	1115.057583	4.966886	-0.016695	1.928657
86.819178	1123.202430	4.971891	-0.016777	1.934671
87.000769	1131.337816	4.976896	-0.016816	1.940633
87.670983	1139.411677	4.981901	-0.016946	1.946586
88.000640	1147.594038	4.986906	-0.017013	1.952561
88.070610	1155.733760	4.991910	-0.017031	1.958460
88.728509	1163.784118	4.996915	-0.017159	1.964340
89.091918	1171.894714	5.001920	-0.017232	1.970214
89.346071	1180.033726	5.006925	-0.017285	1.976078
89.722376	1188.127572	5.011930	-0.017360	1.981907
90.272854	1196.204523	5.016934	-0.017468	1.987724
90.687381	1204.337701	5.021939	-0.017550	1.993550
90.772674	1212.459674	5.026944	-0.017571	1.999316
91.518219	1220.491362	5.031949	-0.017716	2.005071
92.127614	1228.597308	5.036954	-0.017834	2.010847
92.505857	1236.704320	5.041958	-0.017910	2.016584
93.303412	1244.771705	5.046963	-0.018064	2.022319
93.726610	1252.890135	5.051968	-0.018148	2.028035
94.270792	1261.040489	5.056973	-0.018254	2.033770
94.846945	1269.120964	5.061978	-0.018367	2.039443
95.504901	1277.166155	5.066982	-0.018495	2.045084
95.730964	1285.331399	5.071987	-0.018542	2.050749
96.045895	1293.454449	5.076992	-0.018606	2.056378
96.458441	1301.547301	5.081997	-0.018688	2.061980
96.788422	1309.663168	5.087002	-0.018755	2.067575
97.026940	1317.780333	5.092006	-0.018805	2.073146
97.287187	1325.905596	5.097011	-0.018858	2.078710
97.701236	1333.954818	5.102016	-0.018941	2.084222
98.054751	1342.053394	5.107021	-0.019012	2.089748
98.430695	1350.166050	5.112026	-0.019087	2.095270
99.114143	1358.203473	5.117030	-0.019220	2.100757
99.292217	1366.336759	5.122035	-0.019258	2.106245
99.340120	1374.514420	5.127040	-0.019272	2.111736
99.924882	1382.588515	5.132045	-0.019386	2.117195
100.397027	1390.642766	5.137050	-0.019480	2.122615
100.696112	1398.712371	5.142054	-0.019540	2.128016
101.377055	1406.784315	5.147059	-0.019673	2.133440
101.887601	1414.845867	5.152064	-0.019773	2.138828
102.518444	1422.900021	5.157069	-0.019896	2.144209
102.976531	1430.988718	5.162074	-0.019986	2.149582
103.250068	1439.115598	5.167078	-0.020042	2.154949
103.529353	1447.217089	5.172083	-0.020100	2.160287
104.042188	1455.270421	5.177088	-0.020200	2.165602
104.235515	1463.396607	5.182093	-0.020242	2.170922
104.772321	1471.466678	5.187098	-0.020347	2.176224
105.232361	1479.527059	5.192102	-0.020438	2.181500
105.596074	1487.631097	5.197107	-0.020511	2.186782
106.061261	1495.736777	5.202112	-0.020603	2.192061
106.164760	1503.863056	5.207117	-0.020627	2.197308
106.253876	1511.955708	5.212122	-0.020649	2.202520
106.603983	1520.004499	5.217126	-0.020719	2.207715
106.914537	1528.109098	5.222131	-0.020783	2.212930
107.230407	1536.186533	5.227136	-0.020847	2.218115
107.685805	1544.229665	5.232141	-0.020937	2.223279
108.083616	1552.320569	5.237146	-0.021016	2.228456
108.523753	1560.393605	5.242150	-0.021103	2.233614
109.070413	1568.453442	5.247155	-0.021210	2.238760
109.361455	1576.515665	5.252160	-0.021270	2.243874
109.581153	1584.605454	5.257165	-0.021316	2.248987
109.963514	1592.711078	5.262170	-0.021392	2.254112
110.366911	1600.753223	5.267174	-0.021473	2.259188
110.822447	1608.831753	5.272179	-0.021563	2.264279
110.742854	1616.955900	5.277184	-0.021553	2.269341
111.302108	1625.089031	5.282189	-0.021663	2.274453
111.680652	1633.134267	5.287194	-0.021738	2.279483
111.937595	1641.170462	5.292198	-0.021791	2.284485
112.286357	1649.233034	5.297203	-0.021862	2.289501
112.771508	1657.289704	5.302208	-0.021957	2.294514
113.004666	1665.360653	5.307213	-0.022006	2.299503
113.438587	1673.424547	5.312218	-0.022092	2.304494
113.507403	1681.527471	5.317222	-0.022110	2.309467
114.006790	1689.599976	5.322227	-0.022208	2.314447
114.271339	1697.648843	5.327232	-0.022263	2.319382
114.765935	1705.690322	5.332237	-0.022360	2.324321
115.282582	1713.751136	5.337242	-0.022462	2.329263
115.490817	1721.858263	5.342246	-0.022506	2.334198
115.766367	1729.937662	5.347251	-0.022562	2.339110
116.276915	1737.965100	5.352256	-0.022662	2.344000
116.512512	1746.059617	5.357261	-0.022712	2.348898
116.899549	1754.165520	5.362266	-0.022789	2.353804
117.245286	1762.199417	5.367270	-0.022859	2.358654
117.539089	1770.266230	5.372275	-0.022918	2.363509
117.900171	1778.320906	5.377280	-0.022991	2.368352
118.312996	1786.405535	5.382285	-0.023073	2.373208
118.609707	1794.472202	5.387290	-0.023134	2.378033
118.724033	1802.536522	5.392294	-0.023160	2.382833
119.681112	1810.550713	5.397299	-0.023344	2.387660
120.186894	1818.633669	5.402304	-0.023443	2.392482
120.398907	1826.718517	5.407309	-0.023488	2.397272
121.019343	1834.757541	5.412314	-0.023608	2.402058
121.142088	1842.845533	5.417318	-0.023637	2.406824
121.497322	1850.928059	5.422323	-0.023708	2.411595
121.750599	1859.008891	5.427328	-0.023760	2.416348
121.832485	1867.082555	5.432333	-0.023781	2.421074
122.414177	1875.109390	5.437338	-0.023894	2.425802
122.807415	1883.176106	5.442342	-0.023973	2.430530
123.378992	1891.278549	5.447347	-0.024085	2.435282
123.835390	1899.286574	5.452352	-0.024175	2.439962
124.153857	1907.323836	5.457357	-0.024239	2.444639
124.532816	1915.398235	5.462362	-0.024315	2.449333
124.419647	1923.519337	5.467366	-0.024299	2.454008
124.899440	1931.553493	5.472371	-0.024394	2.458669
125.097965	1939.600015	5.477376	-0.024436	2.463306
125.369346	1947.665404	5.482381	-0.024492	2.467951
126.218273	1955.677689	5.487386	-0.024655	2.472600
126.477995	1963.739648	5.492390	-0.024709	2.477225
127.034871	1971.768078	5.497395	-0.024818	2.481844
127.382361	1979.828848	5.502400	-0.024888	2.486457
127.883494	1987.896734	5.507405	-0.024986	2.491076
128.320824	1995.974677	5.512410	-0.025073	2.495689
128.395308	2004.052340	5.517414	-0.025092	2.500265
128.696739	2012.110326	5.522419	-0.025153	2.504839
128.968056	2020.171601	5.527424	-0.025209	2.509405
129.258416	2028.278598	5.532429	-0.025269	2.513988
129.676498	2036.309648	5.537434	-0.025352	2.518530
129.994967	2044.338707	5.542438	-0.025416	2.523056
130.110147	2052.424886	5.547443	-0.025443	2.527591
130.526440	2060.465362	5.552448	-0.025526	2.532113
131.080355	2068.486387	5.557453	-0.025634	2.536626
131.274499	2076.590634	5.562458	-0.025675	2.541152
131.536013	2084.608398	5.567462	-0.025729	2.545627
131.969826	2092.688106	5.572467	-0.025815	2.550140
132.352281	2100.740679	5.577472	-0.025892	2.554627
132.225465	2108.823552	5.582477	-0.025873	2.559086
132.665779	2116.846181	5.587482	-0.025961	2.563545
133.054196	2124.890743	5.592486	-0.026038	2.568003
133.490033	2132.950088	5.597491	-0.026125	2.572466
133.839933	2141.007201	5.602496	-0.026195	2.576913
134.081829	2149.053830	5.607501	-0.026245	2.581340
134.320273	2157.109720	5.612506	-0.026295	2.585764
134.539558	2165.186537	5.617510	-0.026341	2.590190
134.965116	2173.428027	5.622515	-0.026426	2.594712
135.238402	2181.398333	5.627520	-0.026482	2.599069
135.490981	2189.393967	5.632525	-0.026534	2.603430
135.696014	2197.437315	5.637530	-0.026577	2.607807
135.941341	2205.472855	5.642534	-0.026628	2.612175
136.381207	2213.514903	5.647539	-0.026715	2.616552
136.480195	2221.552726	5.652544	-0.026739	2.620897
136.906112	2229.556832	5.657549	-0.026824	2.625238
137.274993	2237.617800	5.662554	-0.026898	2.629599
137.522248	2245.667815	5.667558	-0.026949	2.633938
137.910060	2253.712786	5.672563	-0.027026	2.638277
138.242041	2261.732571	5.677568	-0.027093	2.642592
138.414722	2269.793701	5.682573	-0.027131	2.646911
138.714741	2277.877100	5.687578	-0.027192	2.651243
139.156960	2285.916616	5.692582	-0.027279	2.655554
139.533547	2293.950454	5.697587	-0.027355	2.659850
139.428789	2302.037390	5.702592	-0.027341	2.664137
139.754793	2310.061850	5.707597	-0.027406	2.668411
140.098324	2318.168689	5.712602	-0.027476	2.672723
140.353923	2326.196011	5.717606	-0.027528	2.676981
140.670015	2334.223015	5.722611	-0.027593	2.681235
141.001905	2342.246217	5.727616	-0.027660	2.685481
141.110485	2350.298006	5.732621	-0.027685	2.689722
141.315779	2358.397927	5.737626	-0.027729	2.693987
141.569689	2366.402430	5.742630	-0.027781	2.698199
141.876653	2374.447844	5.747635	-0.027843	2.702429
142.056804	2382.485391	5.752640	-0.027882	2.706640
142.621226	2390.513477	5.757645	-0.027993	2.710863
143.205810	2398.571203	5.762650	-0.028107	2.715096
143.249427	2406.620547	5.767654	-0.028120	2.719285
143.785256	2414.625451	5.772659	-0.028225	2.723475
144.041181	2422.690782	5.777664	-0.028278	2.727672
144.195972	2430.758377	5.782669	-0.028312	2.731858
144.647955	2438.830384	5.787674	-0.028401	2.736058
144.931193	2446.850288	5.792678	-0.028459	2.740214
145.272873	2454.894424	5.797683	-0.028528	2.744379
145.413927	2462.968598	5.802688	-0.028560	2.748542
146.007645	2471.054662	5.807693	-0.028676	2.752732
146.364857	2479.130055	5.812698	-0.028747	2.756895
146.633109	2487.105085	5.817702	-0.028802	2.760995
146.813756	2495.139673	5.822707	-0.028841	2.765115
147.292696	2503.148367	5.827712	-0.028936	2.769233
147.324908	2511.237412	5.832717	-0.028947	2.773359
147.668393	2519.286249	5.837722	-0.029016	2.777477
148.060026	2527.276472	5.842726	-0.029094	2.781562
148.263932	2535.334973	5.847731	-0.029137	2.785664
148.442811	2543.388038	5.852736	-0.029176	2.789756
148.792437	2551.448677	5.857741	-0.029246	2.793856
149.033283	2559.484487	5.862746	-0.029296	2.797931
149.127066	2567.523758	5.867750	-0.029319	2.801993
149.536371	2575.550768	5.872755	-0.029401	2.806061
150.015218	2583.552471	5.877760	-0.029495	2.810115
150.357326	2591.635200	5.882765	-0.029564	2.814195
150.395685	2599.727345	5.887770	-0.029576	2.818257
150.678358	2607.728991	5.892774	-0.029634	2.822281
151.143581	2615.768190	5.897779	-0.029726	2.826329
151.462428	2623.801490	5.902784	-0.029791	2.830360
151.666754	2631.897058	5.907789	-0.029834	2.834410
152.198023	2639.913815	5.912794	-0.029938	2.838433
152.234071	2647.928760	5.917798	-0.029950	2.842421
152.611150	2655.975457	5.922803	-0.030025	2.846439
152.876107	2664.016191	5.927808	-0.030080	2.850441
153.218421	2672.051440	5.932813	-0.030149	2.854440
153.305969	2680.116779	5.937818	-0.030171	2.858434
153.419844	2688.137984	5.942822	-0.030197	2.862402
153.854617	2696.167894	5.947827	-0.030283	2.866386
154.170833	2704.223159	5.952832	-0.030347	2.870370
154.506548	2712.250135	5.957837	-0.030415	2.874337
154.760834	2720.312123	5.962842	-0.030468	2.878310
154.651859	2728.353962	5.967846	-0.030453	2.882248
154.886178	2736.394651	5.972851	-0.030501	2.886199
155.341736	2744.425717	5.977856	-0.030591	2.890152
155.638699	2752.461336	5.982861	-0.030652	2.894093
155.810736	2760.541778	5.987866	-0.030689	2.898043
155.904816	2768.559875	5.992870	-0.030712	2.901954
156.470205	2776.588815	5.997875	-0.030823	2.905890
156.695287	2784.629814	6.002880	-0.030870	2.909808
157.041054	2792.748999	6.007885	-0.030939	2.913765
157.484627	2800.783548	6.012890	-0.031027	2.917681
157.858178	2808.748994	6.017894	-0.031102	2.921554
157.970058	2816.786192	6.022899	-0.031128	2.925444
158.336172	2824.784358	6.027904	-0.031201	2.929322
158.447789	2832.855449	6.032909	-0.031227	2.933217
158.812917	2840.911031	6.037914	-0.031301	2.937113
158.840097	2848.940785	6.042918	-0.031311	2.940973
159.132469	2856.963405	6.047923	-0.031371	2.944839
159.359750	2865.005082	6.052928	-0.031418	2.948705
159.552467	2873.067705	6.057933	-0.031459	2.952574
159.960003	2881.098883	6.062938	-0.031540	2.956435
160.275864	2889.087185	6.067942	-0.031604	2.960265
160.645116	2897.105819	6.072947	-0.031678	2.964107
161.128335	2905.145792	6.077952	-0.031774	2.967960
161.382029	2913.204642	6.082957	-0.031826	2.971806
161.950391	2921.241084	6.087962	-0.031937	2.975651
162.081353	2929.260489	6.092966	-0.031967	2.979462
162.654292	2937.299205	6.097971	-0.032079	2.983299
162.788200	2945.360270	6.102976	-0.032109	2.987119
162.911091	2953.417695	6.107981	-0.032137	2.990932
163.291263	2961.501248	6.112986	-0.032213	2.994766
163.571689	2969.489912	6.117990	-0.032270	2.998545
163.902286	2977.516033	6.122995	-0.032337	3.002339
164.158481	2985.549029	6.128000	-0.032390	3.006128
164.553170	2993.541804	6.133005	-0.032469	3.009900
164.806997	3001.644884	6.138010	-0.032521	3.013712
164.976407	3009.675151	6.143014	-0.032558	3.017481
165.233542	3017.709051	6.148019	-0.032611	3.021251
165.672138	3025.702084	6.153024	-0.032698	3.025006
165.850646	3033.749124	6.158029	-0.032737	3.028769
166.199825	3041.813999	6.163034	-0.032807	3.032544
166.547135	3049.828890	6.168038	-0.032877	3.036290
166.828519	3057.839865	6.173043	-0.032934	3.040027
167.235480	3065.878145	6.178048	-0.033015	3.043778
167.566045	3073.890650	6.183053	-0.033082	3.047509
167.855984	3081.983448	6.188058	-0.033141	3.051271
168.108056	3090.022739	6.193062	-0.033194	3.055001
168.698409	3098.033896	6.198067	-0.033309	3.058729
169.186171	3106.059555	6.203072	-0.033405	3.062455
169.351872	3114.097664	6.208077	-0.033441	3.066167
169.540086	3122.167066	6.213082	-0.033481	3.069890
169.996136	3130.248312	6.218086	-0.033571	3.073626
170.109754	3138.301636	6.223091	-0.033598	3.077328
170.261916	3146.300865	6.228096	-0.033631	3.081004
170.755610	3154.259460	6.233101	-0.033728	3.084672
171.039884	3162.324068	6.238106	-0.033786	3.088374
171.039426	3170.398511	6.243110	-0.033792	3.092063
171.484383	3178.400799	6.248115	-0.033880	3.095736
171.788660	3186.427645	6.253120	-0.033942	3.099408
172.071392	3194.431340	6.258125	-0.033999	3.103065
172.178157	3202.515135	6.263130	-0.034025	3.106746
172.330427	3210.535944	6.268134	-0.034058	3.110396
172.901178	3218.567230	6.273139	-0.034170	3.114065
172.886666	3226.603783	6.278144	-0.034172	3.117706
173.076486	3234.625989	6.283149	-0.034213	3.121345
173.293633	3242.643895	6.288154	-0.034258	3.124980
173.387294	3250.684159	6.293158	-0.034281	3.128614
173.858155	3258.706978	6.298163	-0.034374	3.132254
174.305440	3266.743777	6.303168	-0.034463	3.135894
174.414054	3274.785960	6.308173	-0.034488	3.139517
174.383844	3282.853899	6.313178	-0.034488	3.143142
174.483094	3290.884366	6.318182	-0.034511	3.146751
174.860742	3298.895505	6.323187	-0.034587	3.150360
175.027878	3306.972830	6.328192	-0.034623	3.153985
175.450166	3314.958587	6.333197	-0.034707	3.157576
176.171022	3322.963093	6.338202	-0.034846	3.161184
176.181063	3330.968350	6.343206	-0.034854	3.164758
176.603720	3338.994588	6.348211	-0.034937	3.168354
176.943347	3347.067646	6.353216	-0.035006	3.171964
177.135926	3355.091212	6.358221	-0.035047	3.175541
177.518954	3363.122484	6.363226	-0.035124	3.179126
177.763688	3371.155178	6.368230	-0.035174	3.182701
177.806030	3379.194576	6.373235	-0.035188	3.186267
178.150295	3387.222610	6.378240	-0.035257	3.189836
178.363987	3395.269446	6.383245	-0.035302	3.193404
178.771460	3403.326037	6.388250	-0.035383	3.196981
178.844529	3411.340107	6.393254	-0.035402	3.200520
179.083917	3419.347322	6.398259	-0.035452	3.204060
179.395052	3427.390780	6.403264	-0.035515	3.207615
179.487525	3435.441243	6.408269	-0.035537	3.211160
179.885191	3443.470473	6.413274	-0.035617	3.214704
180.090924	3451.493363	6.418278	-0.035660	3.218233
180.555940	3459.490861	6.423283	-0.035752	3.221758
180.712491	3467.508407	6.428288	-0.035786	3.225275
180.834858	3475.565834	6.433293	-0.035814	3.228805
181.282756	3483.659697	6.438298	-0.035903	3.232360
181.497084	3491.700695	6.443302	-0.035948	3.235878
181.890867	3499.671558	6.448307	-0.036027	3.239369
182.292531	3507.696393	6.453312	-0.036107	3.242880
182.572009	3515.694037	6.458317	-0.036164	3.246370
182.941927	3523.720839	6.463322	-0.036238	3.249873
183.174110	3531.772771	6.468326	-0.036286	3.253377
183.330825	3539.829634	6.473331	-0.036321	3.256877
183.466486	3547.857514	6.478336	-0.036351	3.260360
183.472568	3555.871253	6.483341	-0.036358	3.263827
183.756374	3563.915866	6.488346	-0.036416	3.267316
184.257038	3571.934271	6.493350	-0.036514	3.270797
184.307282	3579.995177	6.498355	-0.036529	3.274276
184.786484	3587.992421	6.503360	-0.036623	3.277740
184.835254	3596.014103	6.508365	-0.036638	3.281194
185.083557	3604.041503	6.513370	-0.036689	3.284655
185.220624	3612.060611	6.518374	-0.036720	3.288104
185.402281	3620.113327	6.523379	-0.036759	3.291566
185.635268	3628.164177	6.528384	-0.036807	3.295025
185.874075	3636.157418	6.533389	-0.036857	3.298456
186.457797	3644.169188	6.538394	-0.036971	3.301905
186.508997	3652.215166	6.543398	-0.036986	3.305344
186.820391	3660.248604	6.548403	-0.037049	3.308784
187.258105	3668.295467	6.553408	-0.037136	3.312231
187.494229	3676.321843	6.558413	-0.037185	3.315658
187.887981	3684.331700	6.563418	-0.037263	3.319080
187.996014	3692.348755	6.568422	-0.037289	3.322491
188.174501	3700.364229	6.573427	-0.037327	3.325901
188.573271	3708.388569	6.578432	-0.037407	3.329319
188.643919	3716.450833	6.583437	-0.037425	3.332737
189.116121	3724.490747	6.588442	-0.037518	3.336157
189.396108	3732.466512	6.593446	-0.037576	3.339540
189.591347	3740.523698	6.598451	-0.037617	3.342950
190.002050	3748.570508	6.603456	-0.037699	3.346360
190.386893	3756.558307	6.608461	-0.037776	3.349741
190.751327	3764.636250	6.613466	-0.037849	3.353155
190.880661	3772.679016	6.618470	-0.037878	3.356543
191.163595	3780.681081	6.623475	-0.037936	3.359916
191.401148	3788.710849	6.628480	-0.037986	3.363295
191.371835	3796.739639	6.633485	-0.037985	3.366661
191.759317	3804.744571	6.638490	-0.038063	3.370028
191.985827	3812.819191	6.643494	-0.038110	3.373416
192.222005	3820.841450	6.648499	-0.038159	3.376778
192.396405	3828.879311	6.653504	-0.038197	3.380141
192.571387	3836.878056	6.658509	-0.038235	3.383485
192.753577	3844.928405	6.663514	-0.038274	3.386847
193.067421	3852.942748	6.668518	-0.038338	3.390196
193.305582	3861.053375	6.673523	-0.038387	3.393578
193.612013	3869.082309	6.678528	-0.038449	3.396925
193.729997	3877.010949	6.683533	-0.038477	3.400221
194.143390	3885.041663	6.688538	-0.038559	3.403566
194.384132	3893.062449	6.693542	-0.038609	3.406898
194.439408	3901.074174	6.698547	-0.038624	3.410217
194.838004	3909.148353	6.703552	-0.038704	3.413569
195.006405	3917.155957	6.708557	-0.038740	3.416883
194.993378	3925.161418	6.713562	-0.038743	3.420187
195.231489	3933.196366	6.718566	-0.038793	3.423508
195.806203	3941.195666	6.723571	-0.038905	3.426823
195.876579	3949.253420	6.728576	-0.038923	3.430141
195.753180	3957.310545	6.733581	-0.038906	3.433450
196.449299	3965.309321	6.738586	-0.039040	3.436758
196.730144	3973.298160	6.743590	-0.039098	3.440046
196.604772	3981.342985	6.748595	-0.039080	3.443339
197.036281	3989.388509	6.753600	-0.039165	3.446649
197.226262	3997.379797	6.758605	-0.039206	3.449925
197.194274	4005.473075	6.763610	-0.039205	3.453232
197.433691	4013.501806	6.768614	-0.039255	3.456518
197.758368	4021.508493	6.773619	-0.039321	3.459796
198.021696	4029.524772	6.778624	-0.039375	3.463071
198.194614	4037.562888	6.783629	-0.039412	3.466350
198.475973	4045.584715	6.788634	-0.039470	3.469623
198.810094	4053.651564	6.793638	-0.039538	3.472912
198.879651	4061.684869	6.798643	-0.039556	3.476176
199.017217	4069.654942	6.803648	-0.039587	3.479414
199.422476	4077.636842	6.808653	-0.039667	3.482661
199.825989	4085.679754	6.813658	-0.039748	3.485931
199.861952	4093.696692	6.818662	-0.039759	3.489175
200.058351	4101.744116	6.823667	-0.039801	3.492433
200.279948	4109.808017	6.828672	-0.039848	3.495696
200.482188	4117.795893	6.833677	-0.039891	3.498925
200.764532	4125.812928	6.838682	-0.039948	3.502164
200.976768	4133.853039	6.843686	-0.039993	3.505408
201.090006	4141.872632	6.848691	-0.040019	3.508637
201.198080	4149.960693	6.853696	-0.040045	3.511891
201.495948	4157.962374	6.858701	-0.040106	3.515113
202.088516	4165.909233	6.863706	-0.040221	3.518319
202.205585	4173.964673	6.868710	-0.040248	3.521551
202.376112	4181.956407	6.873715	-0.040285	3.524756
202.619987	4190.013946	6.878720	-0.040336	3.527987
202.567273	4198.078054	6.883725	-0.040331	3.531208
202.834479	4206.123726	6.888730	-0.040386	3.534429
203.168671	4214.140490	6.893734	-0.040454	3.537637
203.187038	4222.169668	6.898739	-0.040462	3.540837
203.375591	4230.172164	6.903744	-0.040503	3.544030
203.862724	4238.175302	6.908749	-0.040598	3.547228
204.269020	4246.220222	6.913754	-0.040679	3.550438
204.373746	4254.358801	6.918758	-0.040704	3.553673
204.582376	4262.362508	6.923763	-0.040748	3.556855
204.695329	4270.347483	6.928768	-0.040774	3.560023
205.042978	4278.299404	6.933773	-0.040844	3.563183
205.308790	4286.350624	6.938778	-0.040899	3.566376
205.435579	4294.360948	6.943782	-0.040928	3.569546
205.787141	4302.384903	6.948787	-0.040999	3.572726
206.016279	4310.457581	6.953792	-0.041046	3.575918
206.045512	4318.424625	6.958797	-0.041057	3.579060
206.302572	4326.472502	6.963802	-0.041110	3.582238
206.614553	4334.483981	6.968806	-0.041174	3.585400
206.806115	4342.487568	6.973811	-0.041214	3.588552
206.835854	4350.579931	6.978816	-0.041225	3.591732
206.859680	4358.598748	6.983821	-0.041235	3.594881
207.360820	4366.574413	6.988826	-0.041333	3.598023
207.773157	4374.570018	6.993830	-0.041415	3.601167
207.914390	4382.555465	6.998835	-0.041447	3.604297
208.057972	4390.644378	7.003840	-0.041479	3.607465
208.217920	4398.623423	7.008845	-0.041514	3.610588
208.413674	4406.709309	7.013850	-0.041556	3.613750
208.509127	4414.765423	7.018854	-0.041579	3.616896
208.731054	4422.734752	7.023859	-0.041625	3.620008
209.119296	4430.750693	7.028864	-0.041703	3.623140
209.283587	4438.783820	7.033869	-0.041738	3.626270
209.505364	4446.822364	7.038874	-0.041785	3.629401
209.714671	4454.905815	7.043878	-0.041829	3.632547
209.937486	4462.917368	7.048883	-0.041876	3.635662
210.092785	4470.903522	7.053888	-0.041910	3.638763
210.293628	4478.908736	7.058893	-0.041953	3.641870
210.744032	4486.900467	7.063898	-0.042042	3.644975
210.763416	4494.968397	7.068902	-0.042051	3.648096
210.774385	4503.011496	7.073907	-0.042058	3.651204
211.192627	4511.049019	7.078912	-0.042141	3.654318
211.299932	4519.045943	7.083917	-0.042166	3.657406
211.488242	4527.057956	7.088922	-0.042206	3.660499
211.824535	4535.073306	7.093926	-0.042274	3.663594
212.029098	4543.119909	7.098931	-0.042318	3.666696
212.235649	4551.144854	7.103936	-0.042361	3.669786
212.551582	4559.179892	7.108941	-0.042425	3.672881
213.073625	4567.182833	7.113946	-0.042528	3.675966
213.316900	4575.179572	7.118950	-0.042578	3.679038
213.358966	4583.207912	7.123955	-0.042591	3.682115
213.778056	4591.227772	7.128960	-0.042674	3.685196
213.933711	4599.239300	7.133965	-0.042709	3.688264
214.433461	4607.290456	7.138970	-0.042807	3.691354
214.568754	4615.311205	7.143974	-0.042837	3.694420
214.773038	4623.343985	7.148979	-0.042881	3.697490
215.185463	4631.370754	7.153984	-0.042963	3.700560
215.389880	4639.339214	7.158989	-0.043006	3.703600
215.948645	4647.385676	7.163994	-0.043115	3.706676
215.943886	4655.431225	7.168998	-0.043120	3.709736
216.197609	4663.519339	7.174003	-0.043172	3.712815
216.375771	4671.578839	7.179008	-0.043210	3.715879
216.461300	4679.517630	7.184013	-0.043232	3.718892
216.743587	4687.543434	7.189018	-0.043289	3.721941
217.150308	4695.519350	7.194022	-0.043370	3.724971
217.328793	4703.523893	7.199027	-0.043409	3.728004
217.532067	4711.594602	7.204032	-0.043452	3.731060
217.389508	4719.624435	7.209037	-0.043431	3.734090
217.720456	4727.662338	7.214042	-0.043497	3.737132
217.968962	4735.661605	7.219046	-0.043549	3.740155
218.128863	4743.676325	7.224051	-0.043584	3.743179
218.302994	4751.712475	7.229056	-0.043621	3.746208
218.556354	4759.717076	7.234061	-0.043674	3.749226
218.457245	4767.795811	7.239066	-0.043661	3.752260
218.822348	4775.805771	7.244070	-0.043734	3.755278
218.942416	4783.794175	7.249075	-0.043761	3.758278
219.450261	4791.830153	7.254080	-0.043861	3.761304
219.423622	4799.839727	7.259085	-0.043861	3.764304
219.793441	4807.864844	7.264090	-0.043936	3.767317
220.056925	4815.873807	7.269094	-0.043990	3.770319
220.101376	4823.901731	7.274099	-0.044003	3.773321
220.469324	4831.959991	7.279104	-0.044077	3.776339
220.642270	4839.907742	7.284109	-0.044114	3.779309
220.755162	4847.985206	7.289114	-0.044141	3.782324
220.892018	4855.997324	7.294118	-0.044171	3.785312
221.330458	4863.982734	7.299123	-0.044258	3.788295
221.439843	4872.073977	7.304128	-0.044284	3.791307
221.549187	4880.124660	7.309133	-0.044310	3.794302
221.852055	4888.108932	7.314138	-0.044371	3.797274
221.903642	4896.104306	7.319142	-0.044386	3.800243
221.925226	4904.116146	7.324147	-0.044395	3.803214
222.210022	4912.121388	7.329152	-0.044453	3.806187
222.353145	4920.116822	7.334157	-0.044485	3.809150
222.421409	4928.182844	7.339162	-0.044503	3.812136
222.664682	4936.247618	7.344166	-0.044554	3.815122
222.920836	4944.209851	7.349171	-0.044607	3.818069
223.247517	4952.276684	7.354176	-0.044673	3.821053
223.505694	4960.207395	7.359181	-0.044726	3.823983
223.908956	4968.236019	7.364186	-0.044806	3.826951
224.181266	4976.223387	7.369190	-0.044862	3.829897
224.109463	4984.359654	7.374195	-0.044854	3.832890
224.472664	4992.381644	7.379200	-0.044927	3.835846
224.753247	5000.378090	7.384205	-0.044984	3.838790
224.817206	5008.438921	7.389210	-0.045002	3.841750
225.065895	5016.385817	7.394214	-0.045053	3.844670
225.262980	5024.480647	7.399219	-0.045095	3.847641
225.708737	5032.456281	7.404224	-0.045183	3.850571
225.875277	5040.490360	7.409229	-0.045219	3.853514
226.132843	5048.505990	7.414234	-0.045273	3.856451
226.360135	5056.488485	7.419238	-0.045320	3.859372
226.341611	5064.552202	7.424243	-0.045322	3.862316
226.783076	5072.526738	7.429248	-0.045409	3.865234
227.131923	5080.555377	7.434253	-0.045480	3.868168
227.456205	5088.626755	7.439258	-0.045545	3.871114
227.480446	5096.897408	7.444262	-0.045555	3.874125
227.560917	5104.836584	7.449267	-0.045575	3.877014
227.960755	5112.765445	7.454272	-0.045655	3.879904
228.064269	5120.737737	7.459277	-0.045679	3.882801
228.263772	5128.717807	7.464282	-0.045722	3.885700
228.548159	5136.772636	7.469286	-0.045780	3.888627
228.715235	5144.773494	7.474291	-0.045816	3.891529
228.972005	5152.836923	7.479296	-0.045869	3.894453
229.152284	5160.815588	7.484301	-0.045908	3.897343
229.454823	5168.818919	7.489306	-0.045969	3.900242
229.526409	5176.841238	7.494310	-0.045988	3.903142
230.012516	5184.808245	7.499315	-0.046084	3.906027
230.289101	5192.883971	7.504320	-0.046140	3.908945
230.390258	5200.930705	7.509325	-0.046165	3.911847
230.454977	5208.931572	7.514330	-0.046182	3.914730
230.993007	5216.951487	7.519334	-0.046287	3.917626
231.098780	5224.959642	7.524339	-0.046312	3.920508
231.123221	5232.993512	7.529344	-0.046322	3.923396
231.205302	5241.019098	7.534349	-0.046342	3.926279
231.445548	5248.990442	7.539354	-0.046392	3.929144
231.804870	5257.050582	7.544358	-0.046464	3.932041
232.021898	5265.061177	7.549363	-0.046510	3.934915
232.420861	5273.090483	7.554368	-0.046590	3.937797
232.531907	5281.058935	7.559373	-0.046615	3.940650
232.726956	5289.069253	7.564378	-0.046657	3.943517
232.990991	5297.130181	7.569382	-0.046711	3.946401
232.960389	5305.134570	7.574387	-0.046711	3.949258
233.113830	5313.228573	7.579392	-0.046745	3.952148
233.406878	5321.226291	7.584397	-0.046805	3.955004
233.794014	5329.199064	7.589402	-0.046882	3.957851
233.934193	5337.227381	7.594406	-0.046913	3.960711
233.973709	5345.205815	7.599411	-0.046926	3.963549
234.449481	5353.273697	7.604416	-0.047020	3.966425
234.530403	5361.248615	7.609421	-0.047040	3.969259
234.820330	5369.292399	7.614426	-0.047099	3.972119
235.073722	5377.340313	7.619430	-0.047151	3.974977
235.062860	5385.333421	7.624435	-0.047155	3.977810
235.173252	5393.368879	7.629440	-0.047180	3.980657
235.257009	5401.379617	7.634445	-0.047201	3.983494
235.588695	5409.386357	7.639450	-0.047268	3.986331
235.704973	5417.461938	7.644454	-0.047295	3.989186
235.756588	5425.494161	7.649459	-0.047310	3.992024
236.127306	5433.546699	7.654464	-0.047384	3.994871
236.232238	5441.555287	7.659469	-0.047409	3.997697
236.277831	5449.534180	7.664474	-0.047423	4.000509
236.666116	5457.522709	7.669478	-0.047500	4.003328
236.776266	5465.567745	7.674483	-0.047526	4.006161
237.072635	5473.604840	7.679488	-0.047586	4.008992
237.296988	5481.626080	7.684493	-0.047633	4.011814
237.665724	5489.638639	7.689498	-0.047707	4.014633
237.799913	5497.678955	7.694502	-0.047737	4.017456
237.949966	5505.633438	7.699507	-0.047771	4.020248
238.111412	5513.685718	7.704512	-0.047806	4.023071
238.458880	5521.666916	7.709517	-0.047876	4.025871
238.477459	5529.721694	7.714522	-0.047884	4.028690
238.903312	5537.777880	7.719526	-0.047969	4.031513
239.107747	5545.883418	7.724531	-0.048012	4.034348
239.248692	5553.887454	7.729536	-0.048044	4.037145
239.453870	5561.780681	7.734541	-0.048087	4.039902
239.659110	5569.820915	7.739546	-0.048131	4.042708
240.099143	5577.845232	7.744550	-0.048218	4.045510
240.078276	5585.852578	7.749555	-0.048219	4.048298
240.275927	5593.912820	7.754560	-0.048261	4.051105
240.477135	5601.914821	7.759565	-0.048304	4.053891
240.639066	5609.941127	7.764570	-0.048339	4.056682
240.798288	5617.925475	7.769574	-0.048374	4.059456
241.063647	5625.929890	7.774579	-0.048429	4.062237
241.272701	5633.935912	7.779584	-0.048473	4.065016
241.448283	5641.984024	7.784589	-0.048511	4.067807
241.656816	5649.974171	7.789594	-0.048555	4.070577
242.001859	5658.064525	7.794598	-0.048624	4.073381
242.057347	5666.082831	7.799603	-0.048640	4.076154
242.586102	5674.050634	7.804608	-0.048743	4.078915
242.570904	5682.077376	7.809613	-0.048746	4.081686
242.685732	5690.080891	7.814618	-0.048772	4.084449
243.102133	5698.127803	7.819622	-0.048855	4.087230
243.212189	5706.057355	7.824627	-0.048881	4.089964
243.557864	5714.161730	7.829632	-0.048950	4.092759
243.796889	5722.182463	7.834637	-0.049000	4.095522
243.851179	5730.191339	7.839642	-0.049016	4.098277
244.041765	5738.219477	7.844646	-0.049056	4.101039
244.057646	5746.228877	7.849651	-0.049064	4.103790
244.256504	5754.281291	7.854656	-0.049107	4.106556
244.535482	5762.249680	7.859661	-0.049164	4.109292
244.841380	5770.303589	7.864666	-0.049226	4.112056
245.266035	5778.350395	7.869670	-0.049310	4.114818
245.185578	5786.376911	7.874675	-0.049301	4.117564
245.512810	5794.346158	7.879680	-0.049367	4.120294
245.752199	5802.337779	7.884685	-0.049416	4.123028
246.009493	5810.348783	7.889690	-0.049470	4.125768
246.087868	5818.400121	7.894694	-0.049489	4.128517
246.130413	5826.418797	7.899699	-0.049503	4.131253
246.544571	5834.470620	7.904704	-0.049585	4.134003
246.649663	5842.530834	7.909709	-0.049610	4.136750
246.820866	5850.497770	7.914714	-0.049647	4.139464
247.164499	5858.541915	7.919718	-0.049716	4.142205
247.278091	5866.486678	7.924723	-0.049742	4.144907
247.477678	5874.547639	7.929728	-0.049785	4.147648
247.558496	5882.589659	7.934733	-0.049805	4.150380
247.843490	5890.620718	7.939738	-0.049863	4.153108
248.020299	5898.670132	7.944742	-0.049901	4.155840
248.049904	5906.635972	7.949747	-0.049912	4.158539
248.315653	5914.648741	7.954752	-0.049967	4.161256
248.460468	5922.617444	7.959757	-0.049999	4.163954
248.563456	5930.702688	7.964762	-0.050023	4.166689
248.692688	5938.700007	7.969766	-0.050053	4.169394
248.936856	5946.688570	7.974771	-0.050103	4.172095
249.138387	5954.793015	7.979776	-0.050146	4.174832
249.485872	5962.761950	7.984781	-0.050216	4.177524
249.434164	5970.755753	7.989786	-0.050212	4.180218
249.601348	5978.800405	7.994790	-0.050248	4.182930
249.634978	5986.791600	7.999795	-0.050259	4.185620
249.754969	5994.831590	8.004800	-0.050287	4.188326
250.137453	6002.853568	8.009805	-0.050364	4.191028
250.201115	6010.946804	8.014810	-0.050381	4.193748
250.380917	6018.986778	8.019814	-0.050419	4.196449
250.791282	6026.879573	8.024819	-0.050501	4.199102
250.918324	6034.911182	8.029824	-0.050530	4.201796
251.013591	6042.881894	8.034829	-0.050553	4.204468
251.305857	6050.871227	8.039834	-0.050612	4.207147
251.740505	6058.936996	8.044838	-0.050698	4.209851
251.673124	6066.940329	8.049843	-0.050691	4.212527
251.806219	6074.986576	8.054848	-0.050721	4.215218
252.115711	6082.979431	8.059853	-0.050784	4.217891
252.454058	6090.991597	8.064858	-0.050852	4.220569
252.790179	6099.048380	8.069862	-0.050920	4.223260
252.780734	6107.041016	8.074867	-0.050924	4.225925
252.734644	6115.068830	8.079872	-0.050920	4.228599
253.151541	6123.093870	8.084877	-0.051003	4.231276
253.179735	6131.111002	8.089882	-0.051013	4.233944
253.514875	6139.156328	8.094886	-0.051081	4.236622
253.673601	6147.095397	8.099891	-0.051116	4.239262
253.799692	6155.188977	8.104896	-0.051145	4.241952
254.051356	6163.131795	8.109901	-0.051197	4.244590
254.100289	6171.234083	8.114906	-0.051211	4.247278
254.595157	6179.198213	8.119910	-0.051308	4.249923
254.834293	6187.247142	8.124915	-0.051358	4.252592
255.097834	6195.292076	8.129920	-0.051412	4.255258
255.170783	6203.314307	8.134925	-0.051431	4.257912
255.324812	6211.262895	8.139930	-0.051465	4.260542
255.543990	6219.355534	8.144934	-0.051511	4.263218
255.769236	6227.316074	8.149939	-0.051558	4.265849
255.829902	6235.359773	8.154944	-0.051575	4.268505
255.976915	6243.374060	8.159949	-0.051607	4.271149
256.192948	6251.437065	8.164954	-0.051653	4.273809
256.315692	6259.491478	8.169958	-0.051681	4.276463
256.372042	6267.420793	8.174963	-0.051697	4.279074
256.674059	6275.491123	8.179968	-0.051758	4.281732
256.751659	6283.419335	8.184973	-0.051778	4.284339
256.770223	6291.478391	8.189978	-0.051786	4.286988
257.154680	6299.475359	8.194982	-0.051863	4.289617
257.401924	6307.528351	8.199987	-0.051914	4.292262
257.653770	6315.598685	8.204992	-0.051967	4.294911
257.871730	6323.590138	8.209997	-0.052012	4.297532
258.286617	6331.560860	8.215002	-0.052095	4.300147
258.453121	6339.597855	8.220006	-0.052131	4.302779
258.711171	6347.602366	8.225011	-0.052184	4.305400
258.978109	6355.604972	8.230016	-0.052239	4.308019
259.087550	6363.680255	8.235021	-0.052265	4.310658
258.947802	6371.707951	8.240026	-0.052244	4.313279
259.200251	6379.733429	8.245030	-0.052296	4.315900
259.242499	6387.687278	8.250035	-0.052309	4.318495
259.456162	6395.731178	8.255040	-0.052354	4.321119
259.646361	6403.667469	8.260045	-0.052395	4.323706
260.065857	6411.735901	8.265050	-0.052478	4.326336
260.428102	6419.769402	8.270054	-0.052551	4.328952
260.426570	6427.776432	8.275059	-0.052556	4.331556
260.745732	6435.820793	8.280064	-0.052621	4.334172
260.802525	6443.855546	8.285069	-0.052636	4.336782
261.051197	6451.740071	8.290074	-0.052688	4.339343
261.471153	6459.856823	8.295078	-0.052771	4.341979
261.491811	6467.803932	8.300083	-0.052780	4.344556
261.778406	6475.864052	8.305088	-0.052839	4.347169
261.926628	6483.922314	8.310093	-0.052872	4.349780
262.122718	6491.942058	8.315098	-0.052914	4.352376
262.268914	6500.040094	8.320102	-0.052946	4.354996
262.333155	6507.975607	8.325107	-0.052963	4.357562
262.759313	6515.974496	8.330112	-0.053048	4.360148
262.958798	6523.997209	8.335117	-0.053090	4.362739
262.896154	6531.949462	8.340122	-0.053084	4.365305
263.331359	6540.013157	8.345126	-0.053170	4.367908
263.700836	6548.016210	8.350131	-0.053244	4.370489
263.725054	6556.061590	8.355136	-0.053254	4.373080
263.605395	6564.053278	8.360141	-0.053237	4.375652
263.792618	6572.083851	8.365146	-0.053277	4.378236
264.176907	6580.121537	8.370150	-0.053353	4.380822
264.243294	6588.064816	8.375155	-0.053371	4.383375
264.473666	6596.117825	8.380160	-0.053419	4.385962
264.741952	6604.176976	8.385165	-0.053474	4.388550
264.719601	6612.151550	8.390170	-0.053475	4.391107
264.749536	6620.225361	8.395174	-0.053486	4.393696
264.992543	6628.231156	8.400179	-0.053537	4.396262
265.177914	6636.199772	8.405184	-0.053576	4.398814
265.337230	6644.276980	8.410189	-0.053611	4.401399
265.518399	6652.225841	8.415194	-0.053650	4.403942
265.750991	6660.273333	8.420198	-0.053699	4.406515
265.668756	6668.224046	8.425203	-0.053689	4.409054
266.020443	6676.331987	8.430208	-0.053759	4.411644
266.359180	6684.345198	8.435213	-0.053828	4.414202
266.444438	6692.383717	8.440218	-0.053849	4.416766
266.675737	6700.373788	8.445222	-0.053897	4.419313
266.965750	6708.407899	8.450227	-0.053956	4.421873
267.253989	6716.380097	8.455232	-0.054015	4.424412
267.339836	6724.474788	8.460237	-0.054036	4.426987
267.627747	6732.421057	8.465242	-0.054095	4.429515
267.934420	6740.500478	8.470246	-0.054157	4.432083
267.878889	6748.486484	8.475251	-0.054152	4.434619
268.013764	6756.563000	8.480256	-0.054183	4.437183
268.360391	6764.470074	8.485261	-0.054252	4.439692
268.395125	6772.505117	8.490266	-0.054264	4.442240
268.641692	6780.481887	8.495270	-0.054315	4.444768
268.905552	6788.547902	8.500275	-0.054370	4.447323
269.321728	6796.569362	8.505280	-0.054452	4.449863
269.284518	6804.642728	8.510285	-0.054451	4.452416
269.378027	6812.614382	8.515290	-0.054473	4.454936
269.731904	6820.680360	8.520294	-0.054544	4.457486
269.626734	6828.627007	8.525299	-0.054530	4.459994
269.947385	6836.665135	8.530304	-0.054595	4.462532
270.130291	6844.634304	8.535309	-0.054634	4.465046
270.180812	6852.642244	8.540314	-0.054649	4.467570
270.488420	6860.724243	8.545318	-0.054711	4.470117
270.551810	6868.700575	8.550323	-0.054728	4.472628
270.906120	6876.747767	8.555328	-0.054799	4.475161
271.074539	6884.791701	8.560333	-0.054836	4.477691
271.104480	6892.751274	8.565338	-0.054847	4.480193
271.379044	6900.745632	8.570343	-0.054903	4.482705
271.482115	6908.732376	8.575347	-0.054928	4.485212
271.668980	6916.790501	8.580352	-0.054968	4.487741
271.930863	6924.822655	8.585357	-0.055022	4.490261
272.038311	6932.845937	8.590362	-0.055047	4.492775
272.279252	6940.888488	8.595367	-0.055097	4.495295
272.209896	6948.879593	8.600371	-0.055089	4.497797
272.439568	6956.855521	8.605376	-0.055137	4.500293
272.603536	6964.883480	8.610381	-0.055173	4.502803
272.926393	6972.867688	8.615386	-0.055238	4.505299
273.292260	6980.974085	8.620391	-0.055312	4.507832
273.431564	6988.907942	8.625395	-0.055343	4.510309
273.723554	6997.006181	8.630400	-0.055402	4.512837
274.187661	7005.090741	8.635405	-0.055494	4.515358
273.946025	7013.036960	8.640410	-0.055454	4.517834
274.127026	7020.996415	8.645415	-0.055493	4.520314
274.506203	7028.990017	8.650419	-0.055569	4.522803
274.880151	7036.973160	8.655424	-0.055644	4.525287
274.997192	7045.017796	8.660429	-0.055671	4.527789
275.355788	7053.023166	8.665434	-0.055743	4.530278
275.761154	7061.109207	8.670439	-0.055824	4.532790
275.810572	7069.110520	8.675443	-0.055838	4.535274
275.801291	7077.130685	8.680448	-0.055841	4.537762
276.054033	7085.065137	8.685453	-0.055894	4.540223
276.411513	7093.059852	8.690458	-0.055965	4.542701
276.779697	7101.147750	8.695463	-0.056039	4.545207
277.033600	7109.199487	8.700467	-0.056092	4.547700
277.159875	7117.195816	8.705472	-0.056120	4.550174
277.433529	7125.307959	8.710477	-0.056177	4.552683
277.535129	7133.265816	8.715482	-0.056201	4.555142
277.732367	7141.294334	8.720487	-0.056243	4.557622
277.780197	7149.232840	8.725491	-0.056257	4.560073
278.022190	7157.311515	8.730496	-0.056307	4.562566
278.482161	7165.275411	8.735501	-0.056398	4.565022
278.566789	7173.306923	8.740506	-0.056419	4.567498
278.705253	7181.338597	8.745511	-0.056450	4.569972
278.763275	7189.389142	8.750515	-0.056466	4.572451
279.115088	7197.386379	8.755520	-0.056537	4.574912
279.196000	7205.431468	8.760525	-0.056557	4.577386
279.363656	7213.363884	8.765530	-0.056593	4.579824
279.754729	7221.424089	8.770535	-0.056671	4.582300
280.018656	7229.381278	8.775539	-0.056726	4.584744
280.157741	7237.475368	8.780544	-0.056757	4.587228
280.628410	7245.481673	8.785549	-0.056850	4.589683
280.708114	7253.490025	8.790554	-0.056870	4.592138
280.935929	7261.540209	8.795559	-0.056918	4.594605
280.973077	7269.566488	8.800563	-0.056930	4.597062
281.252088	7277.480512	8.805568	-0.056987	4.599484
281.520660	7285.555040	8.810573	-0.057042	4.601954
281.577063	7293.521783	8.815578	-0.057058	4.604390
281.900926	7301.615308	8.820583	-0.057123	4.606863
282.036825	7309.564056	8.825587	-0.057154	4.609290
282.449499	7317.620385	8.830592	-0.057236	4.611749
282.785187	7325.674005	8.835597	-0.057304	4.614205
282.861259	7333.679725	8.840602	-0.057323	4.616646
283.027068	7341.668247	8.845607	-0.057359	4.619080
283.200119	7349.683618	8.850611	-0.057396	4.621522
283.385511	7357.668433	8.855616	-0.057436	4.623952
283.681391	7365.725401	8.860621	-0.057497	4.626403
283.671458	7373.670305	8.865626	-0.057500	4.628819
283.969399	7381.811987	8.870631	-0.057561	4.631293
284.059074	7389.756278	8.875635	-0.057583	4.633706
284.241485	7397.776935	8.880640	-0.057622	4.636141
284.601850	7405.785797	8.885645	-0.057694	4.638571
284.833086	7413.779142	8.890650	-0.057742	4.640995
284.926923	7421.821752	8.895655	-0.057765	4.643432
284.890786	7429.805402	8.900659	-0.057763	4.645851
285.402402	7437.819543	8.905664	-0.057864	4.648277
285.546953	7445.893700	8.910669	-0.057896	4.650720
285.537394	7453.896290	8.915674	-0.057900	4.653141
285.903981	7461.894030	8.920679	-0.057973	4.655558
286.195422	7469.939210	8.925683	-0.058032	4.657989
285.992738	7477.939232	8.930688	-0.058000	4.660405
286.228880	7485.937876	8.935693	-0.058049	4.662819
286.674626	7493.886791	8.940698	-0.058137	4.665216
286.949813	7501.972825	8.945703	-0.058194	4.667654
286.968061	7509.957342	8.950707	-0.058202	4.670060
287.092472	7518.059518	8.955712	-0.058231	4.672500
287.540003	7526.089814	8.960717	-0.058319	4.674917
287.571715	7534.067260	8.965722	-0.058331	4.677317
287.843507	7542.067780	8.970727	-0.058386	4.679723
287.875301	7550.104428	8.975731	-0.058397	4.682138
287.983094	7557.991840	8.980736	-0.058423	4.684507
288.017871	7566.104384	8.985741	-0.058434	4.686943
288.278480	7574.036306	8.990746	-0.058488	4.689323
288.530287	7582.087874	8.995751	-0.058540	4.691738
288.790008	7590.123956	9.000755	-0.058594	4.694146
288.749364	7598.152853	9.005760	-0.058591	4.696552
288.859326	7606.169185	9.010765	-0.058617	4.698953
288.799439	7614.157149	9.015770	-0.058611	4.701344
289.106182	7622.209278	9.020775	-0.058674	4.703752
289.174758	7630.170909	9.025779	-0.058692	4.706133
289.548849	7638.233018	9.030784	-0.058766	4.708541
289.732077	7646.274889	9.035789	-0.058806	4.710943
289.830283	7654.281548	9.040794	-0.058829	4.713333
289.955040	7662.299864	9.045799	-0.058858	4.715725
290.197313	7670.283525	9.050803	-0.058908	4.718106
290.389513	7678.239454	9.055808	-0.058949	4.720477
290.558437	7686.318740	9.060813	-0.058986	4.722884
290.720628	7694.300441	9.065818	-0.059021	4.725260
290.978735	7702.363715	9.070823	-0.059074	4.727660
291.025320	7710.380892	9.075827	-0.059088	4.730045
291.064875	7718.423077	9.080832	-0.059101	4.732436
291.347660	7726.441291	9.085837	-0.059159	4.734818
291.366545	7734.453632	9.090842	-0.059168	4.737198
291.638896	7742.399001	9.095847	-0.059223	4.739556
291.671470	7750.452211	9.100851	-0.059235	4.741945
291.941992	7758.448873	9.105856	-0.059290	4.744316
292.154096	7766.496416	9.110861	-0.059335	4.746701
292.201379	7774.456681	9.115866	-0.059349	4.749059
292.568434	7782.522604	9.120871	-0.059423	4.751447
292.712873	7790.569078	9.125875	-0.059455	4.753828
292.867715	7798.539547	9.130880	-0.059489	4.756185
293.185433	7806.547653	9.135885	-0.059553	4.758552
293.367034	7814.567745	9.140890	-0.059592	4.760922
293.603618	7822.545010	9.145895	-0.059641	4.763277
293.739878	7830.600171	9.150899	-0.059672	4.765655
294.156301	7838.611103	9.155904	-0.059755	4.768017
294.452622	7846.661692	9.160909	-0.059815	4.770391
294.233256	7854.652487	9.165914	-0.059780	4.772747
294.401601	7862.687258	9.170919	-0.059816	4.775114
294.717750	7870.671873	9.175923	-0.059880	4.777464
294.753277	7878.645057	9.180928	-0.059892	4.779811
294.929556	7886.740881	9.185933	-0.059930	4.782192
295.234246	7894.623854	9.190938	-0.059992	4.784509
295.513336	7902.777088	9.195943	-0.060049	4.786904
295.672103	7910.704241	9.200947	-0.060084	4.789232
295.832913	7918.751274	9.205952	-0.060119	4.791595
296.260911	7926.815876	9.210957	-0.060204	4.793959
296.317278	7934.807735	9.215962	-0.060220	4.796303
296.482199	7942.795595	9.220967	-0.060256	4.798645
296.402307	7950.787925	9.225971	-0.060246	4.800987
296.440224	7958.789168	9.230976	-0.060258	4.803330
296.514302	7966.840778	9.235981	-0.060277	4.805687
296.837793	7974.853401	9.240986	-0.060343	4.808030
297.118569	7982.869373	9.245991	-0.060400	4.810373
297.408136	7990.469685	9.250995	-0.060459	4.812594
297.376102	7995.102810	9.256000	-0.060456	4.813948
297.729094	7997.695804	9.261005	-0.060524	4.814704
297.731842	7999.015780	9.266010	-0.060525	4.815089
297.979483	7999.544677	9.271015	-0.060571	4.815242
297.894647	8000.341723	9.276019	-0.060556	4.815476
298.300397	8000.548340	9.281024	-0.060632	4.815534
298.343822	8000.396204	9.286029	-0.060640	4.815489
298.309406	8000.537799	9.291034	-0.060633	4.815531
298.585744	8000.398078	9.296039	-0.060685	4.815489
298.421773	8000.473389	9.301043	-0.060654	4.815512
298.481624	8000.531035	9.306048	-0.060666	4.815528
298.703071	8000.392540	9.311053	-0.060707	4.815487
298.805612	8000.521444	9.316058	-0.060726	4.815524
298.789324	8000.453830	9.321063	-0.060723	4.815504
298.831743	8000.484464	9.326067	-0.060731	4.815513
298.968829	8000.541254	9.331072	-0.060756	4.815529
299.053833	8000.523423	9.336077	-0.060772	4.815523
299.098609	8000.464305	9.341082	-0.060780	4.815506
299.197823	8000.503364	9.346087	-0.060799	4.815517
299.150323	8000.408508	9.351091	-0.060790	4.815489
299.100207	8000.544501	9.356096	-0.060781	4.815529
299.230322	8000.534901	9.361101	-0.060805	4.815526
299.154653	8000.516542	9.366106	-0.060791	4.815521
299.190852	8000.550279	9.371111	-0.060798	4.815530
299.293134	8000.416220	9.376115	-0.060816	4.815491
299.514260	8000.407062	9.381120	-0.060858	4.815487
299.534325	8000.439463	9.386125	-0.060861	4.815496
299.469206	8000.535656	9.391130	-0.060849	4.815525
299.514405	8000.250997	9.396135	-0.060858	4.815441
299.409422	8000.359355	9.401139	-0.060838	4.815473
299.451984	8000.424198	9.406144	-0.060846	4.815492
299.663518	8000.400984	9.411149	-0.060885	4.815484
299.687561	8000.419555	9.416154	-0.060890	4.815490
299.457975	8000.237231	9.421159	-0.060847	4.815438
299.536134	8000.401006	9.426163	-0.060862	4.815485
299.685080	8000.534959	9.431168	-0.060889	4.815523
299.596174	8000.443691	9.436173	-0.060873	4.815497
299.650550	8000.546144	9.441178	-0.060883	4.815527
299.693403	8000.310616	9.446183	-0.060891	4.815458
299.817874	8000.528610	9.451187	-0.060914	4.815521
299.801219	8000.520850	9.456192	-0.060911	4.815519
299.722496	8000.394475	9.461197	-0.060896	4.815482
299.759998	8000.392959	9.466202	-0.060903	4.815482
299.936357	8000.389472	9.471207	-0.060936	4.815480
299.999846	8000.500628	9.476211	-0.060948	4.815512
299.912695	8000.431836	9.481216	-0.060932	4.815492
299.985599	8000.337908	9.486221	-0.060945	4.815464
299.921232	8000.406322	9.491226	-0.060933	4.815485
299.987363	8000.421315	9.496231	-0.060946	4.815489
299.984596	8000.405234	9.501235	-0.060945	4.815484
299.963963	8000.456202	9.506240	-0.060941	4.815499
299.874230	8000.234507	9.511245	-0.060924	4.815435
299.864952	8000.529384	9.516250	-0.060923	4.815521
300.364302	8000.408329	9.521255	-0.061016	4.815483
300.210406	8000.539394	9.526259	-0.060987	4.815522
300.132091	8000.438680	9.531264	-0.060972	4.815493
300.176273	8000.347482	9.536269	-0.060981	4.815466
300.115117	8000.508949	9.541274	-0.060969	4.815514
300.170140	8000.336689	9.546279	-0.060979	4.815463
300.155817	8000.478623	9.551283	-0.060977	4.815505
300.109282	8000.437229	9.556288	-0.060968	4.815493
300.167984	8000.254342	9.561293	-0.060979	4.815439
300.144076	8000.282806	9.566298	-0.060975	4.815448
300.285586	8000.138708	9.571303	-0.061001	4.815405
300.286267	8000.365338	9.576307	-0.061001	4.815471
300.279072	8000.394080	9.581312	-0.061000	4.815479
300.466067	8000.226149	9.586317	-0.061034	4.815429
300.217212	8000.354569	9.591322	-0.060988	4.815468
300.271943	8000.258202	9.596327	-0.060998	4.815440
300.438441	8000.429861	9.601331	-0.061029	4.815489
300.345856	8000.304324	9.606336	-0.061012	4.815453
300.421212	8000.385746	9.611341	-0.061026	4.815476
300.381175	8000.359426	9.616346	-0.061019	4.815469
300.491716	8000.200916	9.621351	-0.061039	4.815422
300.400490	8000.383263	9.626355	-0.061022	4.815476
300.082980	8000.441060	9.631360	-0.060963	4.815494
300.223083	8000.212490	9.636365	-0.060989	4.815427
300.308899	8000.404189	9.641370	-0.061005	4.815482
300.379752	8000.439572	9.646375	-0.061018	4.815492
300.438016	8000.381745	9.651379	-0.061029	4.815475
300.269637	8000.451639	9.656384	-0.060998	4.815496
300.464820	8000.264603	9.661389	-0.061034	4.815441
300.560195	8000.562291	9.666394	-0.061052	4.815527
300.632167	8000.412760	9.671399	-0.061065	4.815483
300.567141	8000.377472	9.676403	-0.061053	4.815473
300.443701	8000.414974	9.681408	-0.061030	4.815485
300.738458	8000.184694	9.686413	-0.061085	4.815416
300.570554	8000.433114	9.691418	-0.061054	4.815489
300.549704	8000.291663	9.696423	-0.061050	4.815448
300.659501	8000.278520	9.701427	-0.061070	4.815444
300.733678	8000.457201	9.706432	-0.061084	4.815496
300.707263	8000.184174	9.711437	-0.061079	4.815416
300.475487	8000.297912	9.716442	-0.061036	4.815450
300.671034	8000.418745	9.721447	-0.061073	4.815485
300.701559	8000.112457	9.726451	-0.061078	4.815395
300.451693	8000.372343	9.731456	-0.061032	4.815472
300.861806	8000.282943	9.736461	-0.061108	4.815444
300.821432	8000.435136	9.741466	-0.061101	4.815489
300.726942	8000.359807	9.746471	-0.061083	4.815467
300.789435	8000.194085	9.751475	-0.061094	4.815419
300.835481	8000.333815	9.756480	-0.061103	4.815459
300.970681	8000.233438	9.761485	-0.061128	4.815429
300.786995	8000.380044	9.766490	-0.061094	4.815473
301.016422	8000.274817	9.771495	-0.061137	4.815441
300.907659	8000.347839	9.776499	-0.061117	4.815463
300.655985	8000.443075	9.781504	-0.061070	4.815492
301.052191	8000.187753	9.786509	-0.061143	4.815415
300.711452	8000.265476	9.791514	-0.061080	4.815440
300.564479	8000.207450	9.796519	-0.061053	4.815424
300.754113	8000.445771	9.801523	-0.061088	4.815492
300.776218	8000.337102	9.806528	-0.061092	4.815460
300.732591	8000.303239	9.811533	-0.061084	4.815451
300.679478	8000.502255	9.816538	-0.061074	4.815509
300.778688	8000.370279	9.821543	-0.061092	4.815470
300.848186	8000.216431	9.826547	-0.061105	4.815425
300.783330	8000.372493	9.831552	-0.061093	4.815471
301.012505	8000.204193	9.836557	-0.061136	4.815420
300.905281	8000.346724	9.841562	-0.061116	4.815463
301.078519	8000.381669	9.846567	-0.061148	4.815472
300.949318	8000.223452	9.851571	-0.061124	4.815426
300.913824	8000.418486	9.856576	-0.061118	4.815483
300.826123	8000.282338	9.861581	-0.061101	4.815444
300.786543	8000.529683	9.866586	-0.061094	4.815517
300.775617	8000.426879	9.871591	-0.061092	4.815487
300.903134	8000.238718	9.876595	-0.061116	4.815431
300.853187	8000.408924	9.881600	-0.061106	4.815481
301.034969	8000.278319	9.886605	-0.061140	4.815442
301.254471	8000.546004	9.891610	-0.061181	4.815519
301.063080	8000.416684	9.896615	-0.061145	4.815482
301.239465	8000.405716	9.901619	-0.061178	4.815478
301.093653	8000.525159	9.906624	-0.061151	4.815514
301.372056	8000.259327	9.911629	-0.061203	4.815435
301.190840	8000.366423	9.916634	-0.061169	4.815467
301.043673	8000.423842	9.921639	-0.061142	4.815484
301.094298	8000.400095	9.926643	-0.061151	4.815477
300.957426	8000.330476	9.931648	-0.061126	4.815458
301.066441	8000.204008	9.936653	-0.061146	4.815420
301.089130	8000.340145	9.941658	-0.061150	4.815460
301.014711	8000.219183	9.946663	-0.061136	4.815425
301.183260	8000.358810	9.951667	-0.061168	4.815465
301.288757	8000.533739	9.956672	-0.061187	4.815515
301.289628	8000.548719	9.961677	-0.061188	4.815520
301.230317	8000.542388	9.966682	-0.061177	4.815518
301.369911	8000.429254	9.971687	-0.061202	4.815484
301.502065	8000.360895	9.976691	-0.061227	4.815464
301.291580	8000.387331	9.981696	-0.061188	4.815473
301.317550	8000.177171	9.986701	-0.061193	4.815411
301.413082	8000.347657	9.991706	-0.061210	4.815460
301.563944	8000.375818	9.996711	-0.061239	4.815468
301.561686	8000.206879	10.001715	-0.061238	4.815419
301.273329	8000.445819	10.006720	-0.061184	4.815490
301.379612	8000.194234	10.011725	-0.061204	4.815416
301.446079	8000.225268	10.016730	-0.061216	4.815424
301.564514	8000.221890	10.021735	-0.061238	4.815423
301.482965	8000.214121	10.026739	-0.061223	4.815421
301.392645	8000.309898	10.031744	-0.061207	4.815449
301.437261	8000.199464	10.036749	-0.061215	4.815417
301.558315	8000.300890	10.041754	-0.061237	4.815446
301.490179	8000.196066	10.046759	-0.061225	4.815416
301.488842	8000.235596	10.051763	-0.061224	4.815427
301.467419	8000.287620	10.056768	-0.061220	4.815443
301.524010	8000.161350	10.061773	-0.061231	4.815405
301.403949	8000.116597	10.066778	-0.061208	4.815393
301.511591	8000.374940	10.071783	-0.061229	4.815468
301.732851	8000.252473	10.076787	-0.061270	4.815431
301.543608	8000.415024	10.081792	-0.061235	4.815479
301.743185	8000.394820	10.086797	-0.061272	4.815473
301.685873	8000.274140	10.091802	-0.061261	4.815438
301.820478	8000.238960	10.096807	-0.061286	4.815427
301.841700	8000.173034	10.101811	-0.061290	4.815407
301.759460	8000.355535	10.106816	-0.061275	4.815461
301.799696	8000.073989	10.111821	-0.061282	4.815379
301.640542	8000.315075	10.116826	-0.061253	4.815450
301.643176	8000.327946	10.121831	-0.061253	4.815454
301.747258	8000.158635	10.126835	-0.061272	4.815404
301.785010	8000.160331	10.131840	-0.061279	4.815404
301.687302	8000.068913	10.136845	-0.061261	4.815378
301.627190	8000.396094	10.141850	-0.061250	4.815473
301.732796	8000.315535	10.146855	-0.061270	4.815449
301.800902	8000.207628	10.151859	-0.061282	4.815418
301.686882	8000.405636	10.156864	-0.061261	4.815476
301.827763	8000.261523	10.161869	-0.061287	4.815433
301.803522	8000.347709	10.166874	-0.061283	4.815459
301.677143	8000.244054	10.171879	-0.061259	4.815429
301.763139	8000.219826	10.176883	-0.061275	4.815421
301.687155	8000.179011	10.181888	-0.061261	4.815410
301.756920	8000.203687	10.186893	-0.061274	4.815417
301.822373	8000.314880	10.191898	-0.061286	4.815449
301.825785	8000.105414	10.196903	-0.061287	4.815388
301.784370	8000.188106	10.201907	-0.061279	4.815412
301.753292	8000.139485	10.206912	-0.061273	4.815398
301.853138	7999.953002	10.211917	-0.061292	4.815343
301.857665	8000.225668	10.216922	-0.061293	4.815423
301.932246	8000.101834	10.221927	-0.061307	4.815386
301.981121	8000.151818	10.226931	-0.061316	4.815400
301.764094	8000.190973	10.231936	-0.061275	4.815413
301.874688	8000.324296	10.236941	-0.061296	4.815451
301.838565	8000.354697	10.241946	-0.061289	4.815460
301.745554	8000.336047	10.246951	-0.061272	4.815455
301.866612	8000.137086	10.251955	-0.061294	4.815397
301.822072	8000.334110	10.256960	-0.061286	4.815454
301.861134	8000.260997	10.261965	-0.061293	4.815433
301.750605	8000.277334	10.266970	-0.061273	4.815438
301.755611	8000.293452	10.271975	-0.061274	4.815443
301.962609	8000.151505	10.276979	-0.061312	4.815400
301.836025	8000.420928	10.281984	-0.061289	4.815480
301.855267	8000.142239	10.286989	-0.061292	4.815398
301.953534	8000.264667	10.291994	-0.061311	4.815434
301.927077	8000.205432	10.296999	-0.061306	4.815416
302.038120	8000.232931	10.302003	-0.061326	4.815424
301.921659	8000.177547	10.307008	-0.061305	4.815408
302.169087	8000.221209	10.312013	-0.061351	4.815420
302.109001	8000.301454	10.317018	-0.061340	4.815444
301.837010	8000.265935	10.322023	-0.061289	4.815434
301.927522	8000.290956	10.327027	-0.061306	4.815441
301.838703	8000.541766	10.332032	-0.061289	4.815515
301.870399	8000.095449	10.337037	-0.061295	4.815385
301.931283	8000.292086	10.342042	-0.061306	4.815442
302.108151	8000.225538	10.347047	-0.061339	4.815421
301.901274	8000.067098	10.352051	-0.061301	4.815376
301.944310	8000.340406	10.357056	-0.061309	4.815456
302.070619	8000.280501	10.362061	-0.061332	4.815438
302.139047	8000.245291	10.367066	-0.061345	4.815427
301.875293	8000.303981	10.372071	-0.061296	4.815445
302.142042	8000.298790	10.377075	-0.061346	4.815443
302.163575	8000.391082	10.382080	-0.061350	4.815469
301.944606	8000.244197	10.387085	-0.061309	4.815428
302.080277	8000.181241	10.392090	-0.061334	4.815409
302.012801	8000.247467	10.397095	-0.061322	4.815428
301.988807	8000.173307	10.402099	-0.061317	4.815407
301.913030	8000.447850	10.407104	-0.061303	4.815487
302.079180	8000.427092	10.412109	-0.061334	4.815480
302.083860	8000.281784	10.417114	-0.061335	4.815438
302.077018	8000.404606	10.422119	-0.061334	4.815474
302.167429	8000.383658	10.427123	-0.061350	4.815467
302.003664	8000.355280	10.432128	-0.061320	4.815460
301.982743	8000.368830	10.437133	-0.061316	4.815464
302.090152	8000.334267	10.442138	-0.061336	4.815453
302.269341	8000.413143	10.447143	-0.061369	4.815475
302.240373	8000.382729	10.452147	-0.061364	4.815467
302.091945	8000.418747	10.457152	-0.061336	4.815478
302.147046	8000.418593	10.462157	-0.061347	4.815478
302.178582	8000.362459	10.467162	-0.061352	4.815461
302.151276	8000.403696	10.472167	-0.061347	4.815473
302.303494	8000.344221	10.477171	-0.061376	4.815455
302.252210	8000.357266	10.482176	-0.061366	4.815459
302.439104	8000.240641	10.487181	-0.061401	4.815424
302.083350	8000.274284	10.492186	-0.061335	4.815436
302.271958	8000.176930	10.497191	-0.061370	4.815406
302.545504	8000.221027	10.502195	-0.061421	4.815418
302.182920	8000.222486	10.507200	-0.061353	4.815420
302.479935	8000.155796	10.512205	-0.061408	4.815399
302.384506	8000.154210	10.517210	-0.061391	4.815399
302.358050	8000.394298	10.522215	-0.061386	4.815469
302.265027	8000.304024	10.527219	-0.061368	4.815444
302.299939	8000.293913	10.532224	-0.061375	4.815440
302.337238	8000.095697	10.537229	-0.061382	4.815382
302.182526	8000.250270	10.542234	-0.061353	4.815428
302.276721	8000.428221	10.547239	-0.061371	4.815480
302.380803	8000.243942	10.552243	-0.061390	4.815425
302.330336	8000.270897	10.557248	-0.061380	4.815434
302.353264	8000.211413	10.562253	-0.061385	4.815416
302.262622	8000.227011	10.567258	-0.061368	4.815421
302.192226	8000.281429	10.572263	-0.061355	4.815437
302.367964	8000.268313	10.577267	-0.061387	4.815433
302.297033	8000.251099	10.582272	-0.061374	4.815428
302.346450	8000.318198	10.587277	-0.061383	4.815447
302.206954	8000.137356	10.592282	-0.061357	4.815395
302.233936	8000.312052	10.597287	-0.061362	4.815446
302.341023	8000.159893	10.602291	-0.061382	4.815401
302.240644	8000.352784	10.607296	-0.061364	4.815458
302.322324	8000.049475	10.612301	-0.061379	4.815369
302.504836	8000.181854	10.617306	-0.061413	4.815407
302.490677	8000.216896	10.622311	-0.061410	4.815417
302.511869	8000.159521	10.627315	-0.061414	4.815400
302.498616	8000.302548	10.632320	-0.061412	4.815442
302.404994	8000.330924	10.637325	-0.061394	4.815451
302.703203	8000.304877	10.642330	-0.061450	4.815442
302.596973	8000.402530	10.647335	-0.061430	4.815471
302.664664	7999.949325	10.652339	-0.061442	4.815338
302.390001	8000.295396	10.657344	-0.061391	4.815440
302.613747	8000.398531	10.662349	-0.061433	4.815469
302.720243	8000.250637	10.667354	-0.061453	4.815426
302.548248	8000.283057	10.672359	-0.061421	4.815436
302.582366	8000.267588	10.677363	-0.061427	4.815431
302.556127	8000.288532	10.682368	-0.061422	4.815438
302.667949	8000.146072	10.687373	-0.061443	4.815395
302.413913	8000.324652	10.692378	-0.061396	4.815449
302.680161	8000.223243	10.697383	-0.061445	4.815418
302.852640	8000.160897	10.702387	-0.061477	4.815399
302.662420	8000.430337	10.707392	-0.061442	4.815478
302.604127	8000.267945	10.712397	-0.061431	4.815431
302.715930	8000.168246	10.717402	-0.061452	4.815402
302.708399	8000.353060	10.722407	-0.061451	4.815456
302.646797	8000.020643	10.727411	-0.061439	4.815359
302.728770	8000.202666	10.732416	-0.061454	4.815412
302.746811	8000.297039	10.737421	-0.061458	4.815439
302.715889	8000.196037	10.742426	-0.061452	4.815410
302.695073	8000.329318	10.747431	-0.061448	4.815449
302.784769	8000.056071	10.752435	-0.061465	4.815369
302.719115	8000.237780	10.757440	-0.061453	4.815422
302.849237	8000.166180	10.762445	-0.061477	4.815400
302.723761	8000.208993	10.767450	-0.061453	4.815414
302.649173	8000.225927	10.772455	-0.061440	4.815419
302.856228	8000.210124	10.777459	-0.061478	4.815413
302.788242	8000.376830	10.782464	-0.061466	4.815462
302.717255	8000.113741	10.787469	-0.061452	4.815386
302.639677	8000.116728	10.792474	-0.061438	4.815387
302.545888	8000.125860	10.797479	-0.061420	4.815390
302.930699	8000.132251	10.802483	-0.061492	4.815390
302.817445	8000.268272	10.807488	-0.061471	4.815430
302.761057	8000.242747	10.812493	-0.061460	4.815423
302.913772	8000.288045	10.817498	-0.061489	4.815436
302.876365	8000.236110	10.822503	-0.061482	4.815421
302.926198	8000.236937	10.827507	-0.061491	4.815421
302.827884	8000.288754	10.832512	-0.061473	4.815436
302.736691	8000.304343	10.837517	-0.061456	4.815441
302.768575	8000.178728	10.842522	-0.061462	4.815404
302.554131	8000.310930	10.847527	-0.061422	4.815444
302.824334	8000.217069	10.852531	-0.061472	4.815415
302.744235	8000.454130	10.857536	-0.061457	4.815485
302.857546	8000.335212	10.862541	-0.061478	4.815450
302.884736	8000.143240	10.867546	-0.061483	4.815394
302.812264	8000.304526	10.872551	-0.061470	4.815441
302.800788	8000.141844	10.877555	-0.061468	4.815394
302.835647	8000.378676	10.882560	-0.061474	4.815463
302.811612	8000.218992	10.887565	-0.061470	4.815416
302.844368	8000.360647	10.892570	-0.061476	4.815457
302.784829	8000.180061	10.897575	-0.061465	4.815405
303.008500	8000.139947	10.902579	-0.061506	4.815392
302.865479	8000.374893	10.907584	-0.061480	4.815461
302.964120	8000.210833	10.912589	-0.061498	4.815413
302.903787	8000.286799	10.917594	-0.061487	4.815435
302.902847	8000.295335	10.922599	-0.061487	4.815438
302.911730	8000.184304	10.927603	-0.061488	4.815405
302.849983	8000.394944	10.932608	-0.061477	4.815467
302.955659	8000.159377	10.937613	-0.061496	4.815398
302.845485	8000.231308	10.942618	-0.061476	4.815419
302.837011	8000.371209	10.947623	-0.061474	4.815460
302.977803	8000.103085	10.952627	-0.061500	4.815381
303.103138	8000.148996	10.957632	-0.061524	4.815394
302.995988	8000.172872	10.962637	-0.061504	4.815402
303.024366	8000.016198	10.967642	-0.061509	4.815356
303.082873	8000.218144	10.972647	-0.061520	4.815414
303.018319	8000.070616	10.977651	-0.061508	4.815372
302.730048	8000.232593	10.982656	-0.061454	4.815420
302.971802	8000.220573	10.987661	-0.061499	4.815416
302.757358	8000.285427	10.992666	-0.061459	4.815436
302.625066	8000.261849	10.997671	-0.061435	4.815429
302.766187	8000.116669	11.002675	-0.061461	4.815386
302.824537	8000.161467	11.007680	-0.061472	4.815399
302.669623	8000.164238	11.012685	-0.061443	4.815401
302.693966	8000.157159	11.017690	-0.061448	4.815399
302.782439	8000.300807	11.022695	-0.061464	4.815440
302.955464	8000.172192	11.027699	-0.061496	4.815402
302.824879	8000.087708	11.032704	-0.061472	4.815378
302.793748	8000.024119	11.037709	-0.061466	4.815359
302.959958	8000.053604	11.042714	-0.061497	4.815367
302.905632	8000.067668	11.047719	-0.061487	4.815371
302.934619	8000.163291	11.052723	-0.061492	4.815399
302.948731	8000.324947	11.057728	-0.061495	4.815446
302.979724	8000.191833	11.062733	-0.061501	4.815407
302.839682	8000.069777	11.067738	-0.061475	4.815372
303.008257	8000.261793	11.072743	-0.061506	4.815428
303.093639	8000.203346	11.077747	-0.061522	4.815410
302.708028	8000.264287	11.082752	-0.061450	4.815430
303.026767	8000.323033	11.087757	-0.061510	4.815445
303.051076	8000.213327	11.092762	-0.061514	4.815413
302.893011	8000.195734	11.097767	-0.061485	4.815409
302.818615	8000.345230	11.102771	-0.061471	4.815453
302.977104	8000.237753	11.107776	-0.061500	4.815421
302.938272	8000.256350	11.112781	-0.061493	4.815426
302.757947	8000.415845	11.117786	-0.061460	4.815474
302.947539	8000.418995	11.122791	-0.061495	4.815474
303.081957	8000.399848	11.127795	-0.061520	4.815468
302.957686	8000.554930	11.132800	-0.061497	4.815513
303.238424	8000.303027	11.137805	-0.061549	4.815439
303.323675	8000.319409	11.142810	-0.061565	4.815443
303.174951	8000.372527	11.147815	-0.061537	4.815459
303.143012	8000.233022	11.152819	-0.061531	4.815419
303.283268	8000.379671	11.157824	-0.061557	4.815461
303.325365	8000.247810	11.162829	-0.061565	4.815422
303.176884	8000.373626	11.167834	-0.061537	4.815459
303.057957	8000.319266	11.172839	-0.061515	4.815444
303.085117	8000.090946	11.177843	-0.061520	4.815377
303.165387	8000.220562	11.182848	-0.061535	4.815415
303.066579	8000.159054	11.187853	-0.061517	4.815397
303.041956	8000.249512	11.192858	-0.061512	4.815424
302.989090	8000.250771	11.197863	-0.061502	4.815424
303.199150	8000.214707	11.202867	-0.061541	4.815413
303.171537	8000.306184	11.207872	-0.061536	4.815440
303.165675	8000.163905	11.212877	-0.061535	4.815398
303.231222	8000.390559	11.217882	-0.061547	4.815464
303.168715	8000.301859	11.222887	-0.061536	4.815439
303.197021	8000.143044	11.227891	-0.061541	4.815392
303.283566	8000.111342	11.232896	-0.061557	4.815382
302.994588	8000.273307	11.237901	-0.061503	4.815431
303.188574	8000.166420	11.242906	-0.061539	4.815399
303.141879	8000.417935	11.247911	-0.061531	4.815473
303.219810	8000.160524	11.252915	-0.061545	4.815397
302.986428	8000.306309	11.257920	-0.061502	4.815441
303.131730	8000.254203	11.262925	-0.061529	4.815425
303.360475	8000.208828	11.267930	-0.061571	4.815410
303.101922	8000.166047	11.272935	-0.061523	4.815399
303.159082	8000.064370	11.277939	-0.061534	4.815369
302.957437	8000.349655	11.282944	-0.061496	4.815454
303.053215	8000.277483	11.287949	-0.061514	4.815432
303.244873	8000.162005	11.292954	-0.061550	4.815397
303.202332	8000.244682	11.297959	-0.061542	4.815422
303.192799	8000.178243	11.302963	-0.061540	4.815402
303.234222	8000.193898	11.307968	-0.061548	4.815407
303.117432	8000.397210	11.312973	-0.061526	4.815467
302.981286	8000.254904	11.317978	-0.061501	4.815426
303.050122	8000.200458	11.322983	-0.061514	4.815409
303.330442	8000.300259	11.327987	-0.061566	4.815437
303.135076	8000.355809	11.332992	-0.061529	4.815454
303.032361	8000.205507	11.337997	-0.061510	4.815411
303.152958	8000.377486	11.343002	-0.061533	4.815461
303.196563	8000.428455	11.348007	-0.061541	4.815475
303.190319	8000.021051	11.353011	-0.061539	4.815356
303.119913	8000.355554	11.358016	-0.061527	4.815454
303.153308	8000.224618	11.363021	-0.061533	4.815416
303.204425	8000.217984	11.368026	-0.061542	4.815414
303.116608	8000.294563	11.373031	-0.061526	4.815437
303.224331	8000.095376	11.378035	-0.061546	4.815378
303.197557	8000.329047	11.383040	-0.061541	4.815446
303.134193	8000.223229	11.388045	-0.061529	4.815416
303.289906	8000.295302	11.393050	-0.061558	4.815436
303.235969	8000.317924	11.398055	-0.061548	4.815443
303.235227	8000.120141	11.403059	-0.061548	4.815385
303.056309	8000.296764	11.408064	-0.061515	4.815438
303.194473	8000.270196	11.413069	-0.061540	4.815429
303.164289	8000.347733	11.418074	-0.061535	4.815452
303.336113	8000.210545	11.423079	-0.061567	4.815411
303.486556	8000.291084	11.428083	-0.061595	4.815434
303.241300	8000.304112	11.433088	-0.061549	4.815439
303.321970	8000.334316	11.438093	-0.061564	4.815447
303.242585	8000.112776	11.443098	-0.061549	4.815383
303.235582	8000.206733	11.448103	-0.061548	4.815410
303.270003	8000.179510	11.453107	-0.061554	4.815402
303.204338	8000.297081	11.458112	-0.061542	4.815437
303.392714	8000.251035	11.463117	-0.061577	4.815423
303.272776	8000.365566	11.468122	-0.061555	4.815457
303.247540	8000.212274	11.473127	-0.061550	4.815412
303.342255	8000.189260	11.478131	-0.061568	4.815405
303.397237	8000.238280	11.483136	-0.061578	4.815419
303.277902	8000.307921	11.488141	-0.061556	4.815440
303.499888	8000.142702	11.493146	-0.061597	4.815390
303.310645	8000.410023	11.498151	-0.061562	4.815469
303.353659	8000.210828	11.503155	-0.061570	4.815411
303.339953	8000.341021	11.508160	-0.061567	4.815449
303.415608	8000.149852	11.513165	-0.061581	4.815393
303.267917	8000.274612	11.518170	-0.061554	4.815430
303.159558	8000.307020	11.523175	-0.061534	4.815440
303.366346	8000.112685	11.528179	-0.061572	4.815382
303.382629	8000.260481	11.533184	-0.061575	4.815425
303.297177	8000.252646	11.538189	-0.061559	4.815424
303.191427	8000.280821	11.543194	-0.061540	4.815432
303.202117	8000.259618	11.548199	-0.061542	4.815426
303.495879	8000.014346	11.553203	-0.061596	4.815353
303.355871	8000.249343	11.558208	-0.061570	4.815422
303.359893	8000.269721	11.563213	-0.061571	4.815428
303.384865	8000.015708	11.568218	-0.061575	4.815354
303.348775	8000.141252	11.573223	-0.061569	4.815391
303.432653	8000.228168	11.578227	-0.061584	4.815416
303.274917	8000.281136	11.583232	-0.061555	4.815432
303.215834	8000.202114	11.588237	-0.061544	4.815409
303.454920	8000.129116	11.593242	-0.061589	4.815387
303.463807	8000.346277	11.598247	-0.061590	4.815450
303.449640	8000.256242	11.603251	-0.061588	4.815424
303.230263	8000.383018	11.608256	-0.061547	4.815462
303.365445	8000.228116	11.613261	-0.061572	4.815416
303.522086	8000.326932	11.618266	-0.061601	4.815444
303.369638	8000.343640	11.623271	-0.061573	4.815450
303.523610	8000.156980	11.628275	-0.061601	4.815395
303.340815	8000.408372	11.633280	-0.061567	4.815469
303.416563	8000.235377	11.638285	-0.061581	4.815418
303.425933	8000.209875	11.643290	-0.061583	4.815410
303.568405	8000.202621	11.648295	-0.061610	4.815408
303.585069	8000.144101	11.653299	-0.061613	4.815390
303.601930	8000.096274	11.658304	-0.061616	4.815376
303.331821	8000.181584	11.663309	-0.061566	4.815403
303.587913	8000.115282	11.668314	-0.061613	4.815382
303.401488	8000.311024	11.673319	-0.061579	4.815440
303.549176	8000.190539	11.678323	-0.061606	4.815404
303.576495	8000.328898	11.683328	-0.061611	4.815444
303.342107	8000.178545	11.688333	-0.061567	4.815402
303.547301	8000.162711	11.693338	-0.061606	4.815396
303.537300	8000.312210	11.698343	-0.061604	4.815440
303.735362	8000.133764	11.703347	-0.061641	4.815387
303.468059	8000.188119	11.708352	-0.061591	4.815404
303.611284	8000.347647	11.713357	-0.061618	4.815450
303.639537	8000.143930	11.718362	-0.061623	4.815390
303.524251	8000.216846	11.723367	-0.061601	4.815412
303.611893	8000.238613	11.728371	-0.061618	4.815418
303.627715	8000.226047	11.733376	-0.061621	4.815414
303.629327	8000.156586	11.738381	-0.061621	4.815394
303.510249	8000.092603	11.743386	-0.061599	4.815376
303.587522	8000.375044	11.748391	-0.061613	4.815458
303.712359	8000.016852	11.753395	-0.061636	4.815353
303.516046	8000.238086	11.758400	-0.061600	4.815418
303.489339	8000.362720	11.763405	-0.061595	4.815455
303.545658	8000.351896	11.768410	-0.061605	4.815451
303.481699	8000.371144	11.773415	-0.061593	4.815457
303.655000	8000.148456	11.778419	-0.061626	4.815391
303.802210	7999.932820	11.783424	-0.061653	4.815328
303.789264	8000.414741	11.788429	-0.061651	4.815468
303.873178	8000.199118	11.793434	-0.061666	4.815405
303.805664	8000.433186	11.798439	-0.061654	4.815474
303.646862	8000.214599	11.803443	-0.061624	4.815411
303.632695	8000.289195	11.808448	-0.061621	4.815433
303.548378	8000.309174	11.813453	-0.061606	4.815439
303.833772	8000.104385	11.818458	-0.061659	4.815378
303.849081	8000.298136	11.823463	-0.061662	4.815434
303.855636	8000.126128	11.828467	-0.061663	4.815384
303.891199	8000.034782	11.833472	-0.061669	4.815357
303.629634	8000.126648	11.838477	-0.061621	4.815385
303.630328	7999.989823	11.843482	-0.061621	4.815345
303.548354	8000.290996	11.848487	-0.061606	4.815434
303.672525	8000.078183	11.853491	-0.061629	4.815371
303.703870	8000.113982	11.858496	-0.061635	4.815381
303.419529	8000.283509	11.863501	-0.061582	4.815432
303.625603	8000.076333	11.868506	-0.061620	4.815370
303.531069	8000.402956	11.873511	-0.061603	4.815466
303.445647	8000.109689	11.878515	-0.061586	4.815381
303.753858	8000.099843	11.883520	-0.061644	4.815377
303.652925	8000.189033	11.888525	-0.061625	4.815403
303.575579	8000.230509	11.893530	-0.061611	4.815416
303.729443	8000.291863	11.898535	-0.061639	4.815433
303.774608	8000.084150	11.903539	-0.061648	4.815372
303.659375	8000.112168	11.908544	-0.061626	4.815381
303.690929	8000.020755	11.913549	-0.061632	4.815354
303.841709	7999.990120	11.918554	-0.061660	4.815344
303.690448	8000.363907	11.923559	-0.061632	4.815454
303.740281	8000.207585	11.928563	-0.061641	4.815408
303.916187	8000.206232	11.933568	-0.061674	4.815407
303.975724	8000.159114	11.938573	-0.061685	4.815393
303.861306	8000.238459	11.943578	-0.061664	4.815417
303.650765	8000.250995	11.948583	-0.061625	4.815421
303.945477	8000.190681	11.953587	-0.061679	4.815402
303.651937	8000.024379	11.958592	-0.061625	4.815355
303.711485	8000.333250	11.963597	-0.061636	4.815445
303.945653	8000.138300	11.968602	-0.061679	4.815387
303.767955	7999.988889	11.973607	-0.061646	4.815344
303.695796	8000.067866	11.978611	-0.061633	4.815368
303.640707	8000.082986	11.983616	-0.061623	4.815372
303.756084	8000.257018	11.988621	-0.061644	4.815423
303.813035	8000.230168	11.993626	-0.061655	4.815414
303.623365	8000.320022	11.998631	-0.061620	4.815442
303.788014	8000.308861	12.003635	-0.061650	4.815438
303.862183	8000.152944	12.008640	-0.061664	4.815392
303.803965	8000.290951	12.013645	-0.061653	4.815432
304.080101	8000.223914	12.018650	-0.061704	4.815411
304.026692	8000.425077	12.023655	-0.061695	4.815470
303.908539	8000.246719	12.028659	-0.061673	4.815419
303.988348	8000.388091	12.033664	-0.061687	4.815460
303.937974	8000.238654	12.038669	-0.061678	4.815416
303.837871	8000.157881	12.043674	-0.061659	4.815393
303.750810	8000.198126	12.048679	-0.061643	4.815405
303.912458	8000.176224	12.053683	-0.061673	4.815398
303.892177	8000.283860	12.058688	-0.061669	4.815430
303.650065	8000.304423	12.063693	-0.061624	4.815437
303.945537	8000.072007	12.068698	-0.061679	4.815368
303.896672	8000.322419	12.073703	-0.061670	4.815441
303.966762	8000.186745	12.078707	-0.061683	4.815401
303.686159	8000.231257	12.083712	-0.061631	4.815415
303.784444	8000.333380	12.088717	-0.061649	4.815445
303.917032	8000.275717	12.093722	-0.061674	4.815427
303.767264	8000.335232	12.098727	-0.061646	4.815445
303.790394	8000.195571	12.103731	-0.061650	4.815404
303.827368	8000.150216	12.108736	-0.061657	4.815391
303.578752	8000.240159	12.113741	-0.061611	4.815419
303.747529	8000.202340	12.118746	-0.061642	4.815407
303.736405	8000.223536	12.123751	-0.061640	4.815413
303.839028	8000.186755	12.128755	-0.061659	4.815402
303.782865	8000.381457	12.133760	-0.061649	4.815459
303.841110	8000.231688	12.138765	-0.061660	4.815415
304.116482	7999.941210	12.143770	-0.061711	4.815329
303.828570	8000.082883	12.148775	-0.061657	4.815371
303.971850	7999.986912	12.153779	-0.061684	4.815343
303.988465	8000.234136	12.158784	-0.061687	4.815415
303.838922	8000.311828	12.163789	-0.061659	4.815438
303.931881	8000.026869	12.168794	-0.061677	4.815355
303.819006	8000.286908	12.173799	-0.061656	4.815431
304.118958	8000.077015	12.178803	-0.061711	4.815368
303.938427	8000.310273	12.183808	-0.061678	4.815437
303.761945	8000.202572	12.188813	-0.061645	4.815407
303.962630	8000.120384	12.193818	-0.061682	4.815382
303.849215	8000.077875	12.198823	-0.061661	4.815370
303.999018	8000.056845	12.203827	-0.061689	4.815363
304.045299	8000.039440	12.208832	-0.061698	4.815358
303.826053	8000.113836	12.213837	-0.061657	4.815380
303.775705	8000.046719	12.218842	-0.061647	4.815361
303.839044	8000.163226	12.223847	-0.061659	4.815395
303.827561	8000.002680	12.228851	-0.061657	4.815348
304.099966	8000.036070	12.233856	-0.061708	4.815356
303.946054	7999.946920	12.238861	-0.061679	4.815331
304.034804	7999.914185	12.243866	-0.061696	4.815321
303.901584	8000.021012	12.248871	-0.061671	4.815353
303.919487	8000.065140	12.253875	-0.061674	4.815366
304.130377	8000.128510	12.258880	-0.061713	4.815383
303.881892	8000.390572	12.263885	-0.061667	4.815461
303.722176	8000.103552	12.268890	-0.061637	4.815378
303.886290	8000.050688	12.273895	-0.061668	4.815362
304.057897	8000.132648	12.278899	-0.061700	4.815385
304.047140	8000.064050	12.283904	-0.061698	4.815365
303.920406	8000.286443	12.288909	-0.061674	4.815430
304.076874	8000.157550	12.293914	-0.061704	4.815392
304.010543	8000.210968	12.298919	-0.061691	4.815408
304.138969	8000.114750	12.303923	-0.061715	4.815379
304.240264	8000.053360	12.308928	-0.061734	4.815361
304.123769	8000.104875	12.313933	-0.061712	4.815376
304.143202	8000.041055	12.318938	-0.061716	4.815358
304.010806	7999.980058	12.323943	-0.061691	4.815340
303.856299	8000.113257	12.328947	-0.061662	4.815380
303.985512	8000.234068	12.333952	-0.061686	4.815415
303.960130	8000.092532	12.338957	-0.061682	4.815374
304.109458	8000.020180	12.343962	-0.061709	4.815352
304.041086	8000.102428	12.348967	-0.061697	4.815376
303.851970	8000.146323	12.353971	-0.061662	4.815390
303.988518	8000.072690	12.358976	-0.061687	4.815368
303.874366	8000.165936	12.363981	-0.061666	4.815395
304.041979	7999.981640	12.368986	-0.061697	4.815341
304.020695	8000.053980	12.373991	-0.061693	4.815362
304.175187	7999.988128	12.378995	-0.061722	4.815342
303.956671	7999.951357	12.384000	-0.061681	4.815332
304.124786	8000.020430	12.389005	-0.061712	4.815352
304.108419	8000.042607	12.394010	-0.061709	4.815358
303.823382	8000.156533	12.399015	-0.061656	4.815393
303.870082	7999.937088	12.404019	-0.061665	4.815329
303.922710	7999.902684	12.409024	-0.061674	4.815318
303.942772	8000.183104	12.414029	-0.061678	4.815400
303.987241	7999.942240	12.419034	-0.061687	4.815330
304.135959	7999.969298	12.424039	-0.061714	4.815337
304.180021	7999.964685	12.429043	-0.061722	4.815335
304.138064	8000.209866	12.434048	-0.061715	4.815407
303.946994	8000.243038	12.439053	-0.061679	4.815418
303.907940	7999.793395	12.444058	-0.061672	4.815286
303.979251	8000.207225	12.449063	-0.061685	4.815407
303.905116	8000.132229	12.454067	-0.061671	4.815385
304.066779	8000.053668	12.459072	-0.061701	4.815362
304.152367	8000.190858	12.464077	-0.061717	4.815401
304.173981	8000.050103	12.469082	-0.061721	4.815360
304.112818	8000.340936	12.474087	-0.061710	4.815445
304.055850	8000.099453	12.479091	-0.061699	4.815375
304.234623	8000.050040	12.484096	-0.061733	4.815360
304.109630	8000.201905	12.489101	-0.061709	4.815405
303.909447	8000.091673	12.494106	-0.061672	4.815374
304.001528	8000.185140	12.499111	-0.061689	4.815400
303.797319	8000.162503	12.504115	-0.061651	4.815395
304.060808	8000.138017	12.509120	-0.061700	4.815386
304.052799	8000.272583	12.514125	-0.061699	4.815426
304.065757	8000.202241	12.519130	-0.061701	4.815405
304.131390	8000.217229	12.524135	-0.061713	4.815409
303.981891	8000.192294	12.529139	-0.061686	4.815403
304.060533	8000.285539	12.534144	-0.061700	4.815429
303.970717	8000.192107	12.539149	-0.061683	4.815403
304.023128	8000.152354	12.544154	-0.061693	4.815391
304.084749	8000.213244	12.549159	-0.061705	4.815408
304.023665	8000.122428	12.554163	-0.061693	4.815382
303.923438	7999.972167	12.559168	-0.061674	4.815339
304.134359	8000.229034	12.564173	-0.061714	4.815413
304.104152	8000.110936	12.569178	-0.061708	4.815378
304.077191	8000.128661	12.574183	-0.061703	4.815384
304.048133	8000.168801	12.579187	-0.061698	4.815395
304.099298	8000.110854	12.584192	-0.061707	4.815378
303.884768	8000.305061	12.589197	-0.061667	4.815436
304.183335	8000.131492	12.594202	-0.061723	4.815384
304.122089	8000.124059	12.599207	-0.061712	4.815382
303.977339	8000.216798	12.604211	-0.061685	4.815410
303.949671	8000.174645	12.609216	-0.061679	4.815398
303.901927	8000.209129	12.614221	-0.061671	4.815408
303.917779	7999.941064	12.619226	-0.061673	4.815330
303.881944	8000.158551	12.624231	-0.061667	4.815393
304.065051	7999.896473	12.629235	-0.061701	4.815316
304.150410	7999.941721	12.634240	-0.061717	4.815329
303.856990	8000.399739	12.639245	-0.061662	4.815464
304.284303	8000.194101	12.644250	-0.061742	4.815402
304.200727	8000.399039	12.649255	-0.061726	4.815462
304.164933	8000.170735	12.654259	-0.061719	4.815395
304.199863	8000.072962	12.659264	-0.061726	4.815367
304.083155	8000.290177	12.664269	-0.061704	4.815431
304.181530	8000.134661	12.669274	-0.061723	4.815385
303.948613	8000.357428	12.674279	-0.061679	4.815451
304.240130	8000.117460	12.679283	-0.061733	4.815380
304.403694	8000.019688	12.684288	-0.061764	4.815350
304.229492	8000.151492	12.689293	-0.061731	4.815390
304.058253	8000.110160	12.694298	-0.061700	4.815378
304.168986	8000.144071	12.699303	-0.061720	4.815388
303.997609	8000.247057	12.704307	-0.061688	4.815419
304.026783	8000.132085	12.709312	-0.061694	4.815385
303.962521	8000.170571	12.714317	-0.061682	4.815396
304.112107	8000.159159	12.719322	-0.061710	4.815392
303.894770	8000.227172	12.724327	-0.061669	4.815413
304.089687	8000.041191	12.729331	-0.061705	4.815358
304.173362	8000.051133	12.734336	-0.061721	4.815360
304.100392	8000.347115	12.739341	-0.061707	4.815447
303.973010	8000.140809	12.744346	-0.061684	4.815388
303.945907	8000.124322	12.749351	-0.061679	4.815383
304.089689	8000.214373	12.754355	-0.061705	4.815409
304.082011	8000.059234	12.759360	-0.061704	4.815363
304.113656	8000.308847	12.764365	-0.061710	4.815436
304.176093	8000.069348	12.769370	-0.061721	4.815366
304.098702	8000.191002	12.774375	-0.061707	4.815402
304.282513	8000.296686	12.779379	-0.061741	4.815432
304.339250	8000.083818	12.784384	-0.061752	4.815369
304.151526	8000.194016	12.789389	-0.061717	4.815402
304.149654	8000.169396	12.794394	-0.061716	4.815395
304.304232	8000.288492	12.799399	-0.061745	4.815429
304.416062	8000.263624	12.804403	-0.061766	4.815421
304.300671	8000.134488	12.809408	-0.061745	4.815384
304.257067	8000.236392	12.814413	-0.061736	4.815414
304.282360	8000.077523	12.819418	-0.061741	4.815368
304.142726	8000.130792	12.824423	-0.061715	4.815384
304.164083	8000.250880	12.829427	-0.061719	4.815419
304.350247	7999.983505	12.834432	-0.061754	4.815340
304.025851	8000.204750	12.839437	-0.061693	4.815406
304.217427	8000.142722	12.844442	-0.061729	4.815387
304.221213	8000.290314	12.849447	-0.061730	4.815430
304.400012	8000.375604	12.854451	-0.061763	4.815454
304.270146	8000.243019	12.859456	-0.061739	4.815416
304.160975	8000.267930	12.864461	-0.061719	4.815424
304.370664	8000.143129	12.869466	-0.061758	4.815386
304.523742	8000.114670	12.874471	-0.061786	4.815377
304.378820	8000.234133	12.879475	-0.061759	4.815413
304.413215	8000.042275	12.884480	-0.061765	4.815357
304.214653	8000.419557	12.889485	-0.061729	4.815468
304.379101	8000.144335	12.894490	-0.061759	4.815387
304.130836	8000.283461	12.899495	-0.061713	4.815429
304.228268	8000.277597	12.904499	-0.061731	4.815426
304.194031	8000.382864	12.909504	-0.061725	4.815457
304.119216	8000.420105	12.914509	-0.061711	4.815468
304.376325	8000.145355	12.919514	-0.061759	4.815387
304.080285	8000.318966	12.924519	-0.061703	4.815439
304.192499	8000.056775	12.929523	-0.061724	4.815362
304.372631	8000.352690	12.934528	-0.061758	4.815448
304.313896	8000.286500	12.939533	-0.061747	4.815429
304.148511	8000.376758	12.944538	-0.061716	4.815456
304.213792	8000.320113	12.949543	-0.061728	4.815439
304.218315	8000.444199	12.954547	-0.061729	4.815475
304.253683	8000.228837	12.959552	-0.061736	4.815412
304.037641	8000.218831	12.964557	-0.061695	4.815410
304.402228	8000.239857	12.969562	-0.061763	4.815414
304.367650	8000.210418	12.974567	-0.061757	4.815406
304.352683	8000.109677	12.979571	-0.061754	4.815377
304.380151	8000.160379	12.984576	-0.061759	4.815391
304.282537	8000.176929	12.989581	-0.061741	4.815397
304.058804	8000.156105	12.994586	-0.061699	4.815392
304.053754	8000.208404	12.999591	-0.061698	4.815407
304.375745	8000.146406	13.004595	-0.061758	4.815387
304.258180	7999.994785	13.009600	-0.061736	4.815344
304.098180	8000.320322	13.014605	-0.061707	4.815439
304.234963	8000.097026	13.019610	-0.061732	4.815374
304.040915	8000.128010	13.024615	-0.061696	4.815384
303.921987	8000.118550	13.029619	-0.061674	4.815381
304.062019	8000.112324	13.034624	-0.061700	4.815379
303.983611	8000.255341	13.039629	-0.061685	4.815421
304.007520	8000.042999	13.044634	-0.061690	4.815359
304.221801	8000.320236	13.049639	-0.061730	4.815439
304.327436	8000.380790	13.054643	-0.061749	4.815456
304.191717	8000.288732	13.059648	-0.061724	4.815430
304.223481	8000.444273	13.064653	-0.061730	4.815475
304.385185	8000.174351	13.069658	-0.061760	4.815395
304.280891	8000.572446	13.074663	-0.061741	4.815512
304.091696	8000.429252	13.079667	-0.061705	4.815471
304.299862	8000.208210	13.084672	-0.061744	4.815406
304.324737	8000.348669	13.089677	-0.061749	4.815447
304.380415	8000.213824	13.094682	-0.061759	4.815407
304.241080	8000.248924	13.099687	-0.061733	4.815418
304.184217	8000.231942	13.104691	-0.061723	4.815413
304.271810	8000.020658	13.109696	-0.061739	4.815351
304.181722	8000.327046	13.114701	-0.061722	4.815441
304.488283	8000.309692	13.119706	-0.061779	4.815434
304.290477	8000.104352	13.124711	-0.061742	4.815375
304.113179	8000.162340	13.129715	-0.061709	4.815393
304.082865	8000.314710	13.134720	-0.061704	4.815438
304.208372	8000.303967	13.139725	-0.061727	4.815434
304.098352	8000.347038	13.144730	-0.061707	4.815447
304.181342	8000.051221	13.149735	-0.061722	4.815360
304.289986	8000.299977	13.154739	-0.061742	4.815433
304.288754	8000.159910	13.159744	-0.061742	4.815392
304.132941	8000.187253	13.164749	-0.061713	4.815400
304.222398	8000.072213	13.169754	-0.061729	4.815366
304.394207	8000.126382	13.174759	-0.061762	4.815381
304.363211	8000.323642	13.179763	-0.061756	4.815439
304.341710	8000.248450	13.184768	-0.061752	4.815417
304.255854	8000.378516	13.189773	-0.061736	4.815456
304.240449	8000.372914	13.194778	-0.061733	4.815454
304.188043	8000.310037	13.199783	-0.061723	4.815436
303.955567	8000.331829	13.204787	-0.061680	4.815444
304.250044	8000.256545	13.209792	-0.061735	4.815420
304.096219	8000.277506	13.214797	-0.061706	4.815427
304.154334	8000.269919	13.219802	-0.061717	4.815424
304.164672	8000.169600	13.224807	-0.061719	4.815395
304.155719	8000.259251	13.229811	-0.061717	4.815421
304.399547	8000.111498	13.234816	-0.061762	4.815377
304.143868	8000.153217	13.239821	-0.061715	4.815390
304.346641	8000.058234	13.244826	-0.061753	4.815362
304.254338	8000.219195	13.249831	-0.061735	4.815409
304.156233	8000.128833	13.254835	-0.061717	4.815383
304.326328	8000.186181	13.259840	-0.061749	4.815399
304.175680	8000.130224	13.264845	-0.061721	4.815384
304.195356	8000.318703	13.269850	-0.061724	4.815439
304.218599	8000.176905	13.274855	-0.061729	4.815397
304.120415	8000.198792	13.279859	-0.061710	4.815404
304.302231	8000.095977	13.284864	-0.061744	4.815373
304.115357	8000.150599	13.289869	-0.061709	4.815390
304.157222	8000.339448	13.294874	-0.061717	4.815445
304.215636	8000.313692	13.299879	-0.061728	4.815437
304.243912	8000.320576	13.304883	-0.061733	4.815439
304.471396	8000.119098	13.309888	-0.061776	4.815379
304.340273	8000.308279	13.314893	-0.061751	4.815435
304.233257	8000.009304	13.319898	-0.061731	4.815348
304.407775	8000.060311	13.324903	-0.061764	4.815362
304.137629	8000.231144	13.329907	-0.061714	4.815413
304.293251	8000.066959	13.334912	-0.061742	4.815365
304.163722	8000.144984	13.339917	-0.061718	4.815388
304.172313	7999.945215	13.344922	-0.061720	4.815330
304.321080	8000.190360	13.349927	-0.061748	4.815400
304.328739	8000.196901	13.354931	-0.061749	4.815402
304.349617	8000.124552	13.359936	-0.061753	4.815381
304.193209	8000.247031	13.364941	-0.061724	4.815418
304.308530	8000.182666	13.369946	-0.061745	4.815398
304.408548	8000.388519	13.374951	-0.061764	4.815458
304.240378	8000.316233	13.379955	-0.061733	4.815438
304.060087	8000.361342	13.384960	-0.061699	4.815452
304.029997	8000.269972	13.389965	-0.061694	4.815425
304.220229	8000.060393	13.394970	-0.061729	4.815363
304.207949	8000.172438	13.399975	-0.061727	4.815396
304.246861	8000.201949	13.404979	-0.061734	4.815404
304.444923	8000.240520	13.409984	-0.061771	4.815414
304.244104	8000.267114	13.414989	-0.061733	4.815423
304.210103	8000.394836	13.419994	-0.061727	4.815461
304.448399	8000.427662	13.424999	-0.061771	4.815469
304.409279	8000.408837	13.430003	-0.061764	4.815464
304.352434	7999.944992	13.435008	-0.061753	4.815329
304.431764	8000.312994	13.440013	-0.061768	4.815436
304.347956	8000.269907	13.445018	-0.061753	4.815424
304.178345	8000.422100	13.450023	-0.061721	4.815469
304.102444	8000.432597	13.455027	-0.061707	4.815472
304.296894	8000.253020	13.460032	-0.061743	4.815419
304.347105	8000.460184	13.465037	-0.061753	4.815479
304.266095	8000.433179	13.470042	-0.061738	4.815472
304.398421	8000.218359	13.475047	-0.061762	4.815408
304.155086	8000.401398	13.480051	-0.061717	4.815463
304.145320	8000.124350	13.485056	-0.061715	4.815382
304.136367	8000.281351	13.490061	-0.061713	4.815428
304.233870	8000.172859	13.495066	-0.061731	4.815396
304.388397	8000.374272	13.500071	-0.061760	4.815454
304.297590	8000.302204	13.505075	-0.061743	4.815433
304.261373	8000.336880	13.510080	-0.061737	4.815444
304.387539	8000.347530	13.515085	-0.061760	4.815446
304.300853	8000.288359	13.520090	-0.061744	4.815429
304.292873	8000.234773	13.525095	-0.061742	4.815414
304.334640	8000.294265	13.530099	-0.061750	4.815431
304.206814	8000.192717	13.535104	-0.061726	4.815402
304.135508	8000.304851	13.540109	-0.061713	4.815435
304.346777	8000.237805	13.545114	-0.061752	4.815414
304.432985	8000.279862	13.550119	-0.061768	4.815426
304.158797	8000.250714	13.555123	-0.061717	4.815419
304.434147	8000.310883	13.560128	-0.061769	4.815435
304.272373	8000.132868	13.565133	-0.061738	4.815384
304.213084	8000.367073	13.570138	-0.061727	4.815453
304.260379	8000.149772	13.575143	-0.061736	4.815389
304.414969	8000.280628	13.580147	-0.061765	4.815426
304.344098	8000.149024	13.585152	-0.061752	4.815388
304.239298	8000.429513	13.590157	-0.061732	4.815471
304.415066	8000.280628	13.595162	-0.061765	4.815426
304.501735	8000.266032	13.600167	-0.061781	4.815422
304.279155	8000.297610	13.605171	-0.061740	4.815432
304.186529	8000.108986	13.610176	-0.061722	4.815377
304.348750	8000.237830	13.615181	-0.061753	4.815414
304.374683	8000.128148	13.620186	-0.061757	4.815382
304.396758	8000.095374	13.625191	-0.061761	4.815372
304.578727	8000.203165	13.630195	-0.061795	4.815403
304.469055	8000.027086	13.635200	-0.061775	4.815352
304.250816	8000.195575	13.640205	-0.061734	4.815402
304.513228	8000.104791	13.645210	-0.061783	4.815375
304.374069	8000.097132	13.650215	-0.061757	4.815373
304.159901	8000.082882	13.655219	-0.061717	4.815370
304.297302	8000.102269	13.660224	-0.061743	4.815375
304.317278	8000.272580	13.665229	-0.061747	4.815424
304.154935	8000.159769	13.670234	-0.061716	4.815392
304.137419	8000.143441	13.675239	-0.061713	4.815388
304.378496	8000.182727	13.680243	-0.061758	4.815398
304.428822	8000.087348	13.685248	-0.061767	4.815370
304.132831	8000.194678	13.690253	-0.061712	4.815403
304.247283	8000.183751	13.695258	-0.061734	4.815399
304.293778	8000.255081	13.700263	-0.061742	4.815419
304.056643	8000.238310	13.705267	-0.061698	4.815416
304.333901	8000.247194	13.710272	-0.061750	4.815417
304.465037	8000.155297	13.715277	-0.061774	4.815390
304.387381	8000.390268	13.720282	-0.061760	4.815459
304.323823	8000.257716	13.725287	-0.061748	4.815420
304.356523	8000.220842	13.730291	-0.061754	4.815409
304.376468	8000.115337	13.735296	-0.061758	4.815378
304.229548	8000.184520	13.740301	-0.061730	4.815399
304.364486	8000.248768	13.745306	-0.061755	4.815417
304.479612	8000.112773	13.750311	-0.061777	4.815377
304.240996	8000.429523	13.755315	-0.061732	4.815471
304.310880	8000.322709	13.760320	-0.061745	4.815439
304.385989	8000.354960	13.765325	-0.061759	4.815448
304.384315	8000.370968	13.770330	-0.061759	4.815453
304.372730	8000.104580	13.775335	-0.061757	4.815375
304.469437	8000.306100	13.780339	-0.061775	4.815434
304.484652	8000.234726	13.785344	-0.061778	4.815413
304.196815	8000.265219	13.790349	-0.061724	4.815423
304.239410	8000.372832	13.795354	-0.061732	4.815454
304.382454	8000.374141	13.800359	-0.061759	4.815454
304.350081	8000.298768	13.805363	-0.061753	4.815432
304.418745	8000.143827	13.810368	-0.061765	4.815386
304.387693	8000.319704	13.815373	-0.061760	4.815438
304.362813	8000.424058	13.820378	-0.061755	4.815468
304.460275	8000.289907	13.825383	-0.061773	4.815429
304.573204	8000.294991	13.830387	-0.061794	4.815430
304.701500	8000.370890	13.835392	-0.061818	4.815451
304.357714	8000.084011	13.840397	-0.061754	4.815369
304.339539	8000.061259	13.845402	-0.061750	4.815363
304.315800	7999.951822	13.850407	-0.061746	4.815331
304.323568	8000.099478	13.855411	-0.061748	4.815374
304.422898	8000.150305	13.860416	-0.061766	4.815388
304.314924	8000.184857	13.865421	-0.061746	4.815399
304.446326	8000.376265	13.870426	-0.061771	4.815454
304.423736	8000.125729	13.875431	-0.061766	4.815381
304.446799	8000.386962	13.880435	-0.061771	4.815457
304.585947	8000.184015	13.885440	-0.061796	4.815397
304.301430	8000.328953	13.890445	-0.061744	4.815441
304.349470	8000.153356	13.895450	-0.061752	4.815390
304.406866	8000.208832	13.900455	-0.061763	4.815405
304.617420	8000.248680	13.905459	-0.061802	4.815416
304.601760	8000.053851	13.910464	-0.061799	4.815359
304.530893	8000.055879	13.915469	-0.061786	4.815360
304.462716	8000.232208	13.920474	-0.061773	4.815412
304.451772	8000.239509	13.925479	-0.061771	4.815414
304.265538	8000.463054	13.930483	-0.061737	4.815480
304.641655	8000.243734	13.935488	-0.061807	4.815414
304.402140	8000.285721	13.940493	-0.061762	4.815428
304.396847	8000.340155	13.945498	-0.061761	4.815444
304.466574	8000.180954	13.950503	-0.061774	4.815397
304.292664	8000.229378	13.955507	-0.061742	4.815412
304.346949	8000.125512	13.960512	-0.061752	4.815381
304.450149	8000.163575	13.965517	-0.061771	4.815392
304.564900	8000.104546	13.970522	-0.061792	4.815374
304.241567	8000.037167	13.975527	-0.061732	4.815356
304.367775	8000.320424	13.980531	-0.061756	4.815438
304.341400	8000.028134	13.985536	-0.061751	4.815353
304.399986	8000.065455	13.990541	-0.061762	4.815364
304.506872	8000.158100	13.995546	-0.061782	4.815390
304.423318	8000.094706	14.000551	-0.061766	4.815372
304.341934	8000.122217	14.005555	-0.061751	4.815380
304.404416	8000.116841	14.010560	-0.061762	4.815379
304.389954	7999.984038	14.015565	-0.061760	4.815340
304.345201	8000.174653	14.020570	-0.061751	4.815396
304.352576	8000.082837	14.025575	-0.061753	4.815369
304.324997	8000.276945	14.030579	-0.061748	4.815426
304.530341	8000.173453	14.035584	-0.061786	4.815395
304.436458	8000.171892	14.040589	-0.061768	4.815395
304.338421	8000.234405	14.045594	-0.061750	4.815413
304.582035	8000.162551	14.050599	-0.061795	4.815391
304.449994	8000.321783	14.055603	-0.061771	4.815438
304.324720	8000.239521	14.060608	-0.061748	4.815415
304.370174	8000.256312	14.065613	-0.061756	4.815419
304.516650	8000.220260	14.070618	-0.061783	4.815408
304.457313	8000.243861	14.075623	-0.061772	4.815415
304.275682	8000.200217	14.080627	-0.061738	4.815404
304.294141	7999.905468	14.085632	-0.061742	4.815317
304.458488	8000.182943	14.090637	-0.061772	4.815398
304.591417	8000.215086	14.095642	-0.061797	4.815406
304.590158	8000.104952	14.100647	-0.061797	4.815374
304.622854	8000.121530	14.105651	-0.061803	4.815379
304.670194	8000.183253	14.110656	-0.061812	4.815397
304.642607	8000.199899	14.115661	-0.061807	4.815402
304.612768	8000.134190	14.120666	-0.061801	4.815383
304.676822	8000.046523	14.125671	-0.061813	4.815357
304.539766	8000.238812	14.130675	-0.061788	4.815414
304.629964	8000.016878	14.135680	-0.061804	4.815348
304.444998	8000.154918	14.140685	-0.061770	4.815390
304.372469	8000.190060	14.145690	-0.061756	4.815400
304.605096	8000.098780	14.150695	-0.061800	4.815372
304.611067	8000.250685	14.155699	-0.061801	4.815417
304.663452	8000.188481	14.160704	-0.061810	4.815398
304.589131	8000.204350	14.165709	-0.061797	4.815403
304.642159	8000.167814	14.170714	-0.061807	4.815392
304.583540	8000.143320	14.175719	-0.061796	4.815385
304.535891	8000.263331	14.180723	-0.061787	4.815421
304.555223	8000.146055	14.185728	-0.061790	4.815386
304.537602	8000.249460	14.190733	-0.061787	4.815417
304.477158	8000.237764	14.195738	-0.061776	4.815414
304.646668	7999.960489	14.200743	-0.061807	4.815332
304.738229	8000.217515	14.205747	-0.061824	4.815406
304.745817	8000.147083	14.210752	-0.061826	4.815386
304.603320	8000.142575	14.215757	-0.061799	4.815385
304.620010	8000.136438	14.220762	-0.061802	4.815383
304.743979	8000.108564	14.225767	-0.061825	4.815375
304.464114	8000.294204	14.230771	-0.061773	4.815430
304.577084	8000.033093	14.235776	-0.061794	4.815353
304.750910	8000.289350	14.240781	-0.061827	4.815427
304.705244	8000.022394	14.245786	-0.061818	4.815350
304.765151	8000.004146	14.250791	-0.061829	4.815344
304.677779	8000.095701	14.255795	-0.061813	4.815371
304.741477	7999.503444	14.260800	-0.061824	4.815198
304.378238	7996.301385	14.265805	-0.061755	4.814264
304.573360	7990.705021	14.270810	-0.061787	4.812628
304.740261	7983.980062	14.275815	-0.061814	4.810662
304.423300	7976.665016	14.280819	-0.061750	4.808525
304.240064	7969.018281	14.285824	-0.061711	4.806289
304.368490	7961.227554	14.290829	-0.061730	4.804008
304.309364	7953.286210	14.295834	-0.061714	4.801683
304.257415	7945.397865	14.300839	-0.061699	4.799373
304.345411	7937.429199	14.305843	-0.061710	4.797037
304.497081	7929.427019	14.310848	-0.061733	4.794690
304.149751	7921.364976	14.315853	-0.061663	4.792326
304.228479	7913.349395	14.320858	-0.061673	4.789973
304.216506	7905.424651	14.325863	-0.061665	4.787646
304.197962	7897.378322	14.330867	-0.061657	4.785282
304.164414	7889.397362	14.335872	-0.061645	4.782936
304.263275	7881.438078	14.340877	-0.061658	4.780595
304.148570	7873.395969	14.345882	-0.061632	4.778229
304.271103	7865.402414	14.350887	-0.061649	4.775875
304.211938	7857.397653	14.355891	-0.061633	4.773518
304.112450	7849.311619	14.360896	-0.061609	4.771135
303.894856	7841.376374	14.365901	-0.061564	4.768797
303.955626	7833.341745	14.370906	-0.061570	4.766427
304.054573	7825.380315	14.375911	-0.061583	4.764077
303.962449	7817.376056	14.380915	-0.061561	4.761714
303.875141	7809.365306	14.385920	-0.061539	4.759347
304.154004	7801.423102	14.390925	-0.061586	4.756999
303.943767	7793.354488	14.395930	-0.061541	4.754614
303.924551	7785.320679	14.400935	-0.061533	4.752237
303.830304	7777.234177	14.405939	-0.061510	4.749844
303.760057	7769.349144	14.410944	-0.061492	4.747509
303.520208	7761.297643	14.415949	-0.061442	4.745124
303.459265	7753.374326	14.420954	-0.061425	4.742775
303.686231	7745.311701	14.425959	-0.061462	4.740383
303.799272	7737.298178	14.430963	-0.061478	4.738005
303.702696	7729.338047	14.435968	-0.061455	4.735642
303.637856	7721.285579	14.440973	-0.061437	4.733250
303.610436	7713.282737	14.445978	-0.061427	4.730872
303.616363	7705.333589	14.450983	-0.061423	4.728508
303.430025	7697.307949	14.455987	-0.061383	4.726121
303.525794	7689.341442	14.460992	-0.061396	4.723749
303.345691	7681.353392	14.465997	-0.061357	4.721371
303.448521	7673.300675	14.471002	-0.061371	4.718971
303.660513	7665.354516	14.476007	-0.061405	4.716602
303.449536	7657.272710	14.481011	-0.061361	4.714192
303.390717	7649.273765	14.486016	-0.061344	4.711806
303.387412	7641.282481	14.491021	-0.061339	4.709420
303.267605	7633.275547	14.496026	-0.061311	4.707028
303.131492	7625.301856	14.501031	-0.061281	4.704646
303.148888	7617.309385	14.506035	-0.061279	4.702256
303.121198	7609.323787	14.511040	-0.061268	4.699867
303.124936	7601.348744	14.516045	-0.061264	4.697480
302.979074	7593.293369	14.521050	-0.061231	4.695068
303.061776	7585.235369	14.526055	-0.061241	4.692653
302.900595	7577.215336	14.531059	-0.061206	4.690249
302.921768	7569.296351	14.536064	-0.061205	4.687874
302.986518	7561.240189	14.541069	-0.061212	4.685456
302.973796	7553.289595	14.546074	-0.061204	4.683069
302.976428	7545.278736	14.551079	-0.061199	4.680663
302.746550	7537.267629	14.556083	-0.061151	4.678255
302.994511	7529.269465	14.561088	-0.061192	4.675850
302.975881	7521.248055	14.566093	-0.061184	4.673436
302.790161	7513.128382	14.571098	-0.061144	4.670993
302.645227	7505.219459	14.576103	-0.061112	4.668611
302.769853	7497.189466	14.581107	-0.061130	4.666191
302.780304	7489.250077	14.586112	-0.061126	4.663797
302.873759	7481.226117	14.591117	-0.061139	4.661377
302.906796	7473.218475	14.596122	-0.061139	4.658960
302.840505	7465.273537	14.601127	-0.061122	4.656561
302.809580	7457.231605	14.606131	-0.061111	4.654132
302.618134	7449.198528	14.611136	-0.061070	4.651704
302.520781	7441.176211	14.616141	-0.061047	4.649277
302.406306	7433.195212	14.621146	-0.061020	4.646863
302.514241	7425.210768	14.626151	-0.061035	4.644445
302.434980	7417.228947	14.631155	-0.061015	4.642027
302.431965	7409.207215	14.636160	-0.061009	4.639596
302.382759	7401.298710	14.641165	-0.060995	4.637198
302.389139	7393.182497	14.646170	-0.060991	4.634736
302.340071	7385.219604	14.651175	-0.060977	4.632319
302.281016	7377.115972	14.656179	-0.060960	4.629858
302.187819	7369.186116	14.661184	-0.060938	4.627448
302.264187	7361.148728	14.666189	-0.060947	4.625005
302.084588	7353.166625	14.671194	-0.060908	4.622577
302.240144	7345.176744	14.676199	-0.060932	4.620145
302.051943	7337.196971	14.681203	-0.060892	4.617715
301.971053	7329.164151	14.686208	-0.060871	4.615268
302.077717	7321.213483	14.691213	-0.060886	4.612844
301.951644	7313.125739	14.696218	-0.060857	4.610378
301.867956	7305.188634	14.701223	-0.060836	4.607956
301.847626	7297.128956	14.706227	-0.060827	4.605495
301.898006	7289.173690	14.711232	-0.060832	4.603065
302.010251	7281.170484	14.716237	-0.060847	4.600619
301.838777	7273.142179	14.721242	-0.060810	4.598163
302.025414	7265.142299	14.726247	-0.060840	4.595716
301.985485	7257.090852	14.731251	-0.060827	4.593251
301.635153	7249.093147	14.736256	-0.060756	4.590801
301.714676	7241.112341	14.741261	-0.060766	4.588355
301.666300	7233.123802	14.746266	-0.060752	4.585906
301.635880	7225.154781	14.751271	-0.060741	4.583461
301.480887	7217.088642	14.756275	-0.060707	4.580985
301.488400	7209.112903	14.761280	-0.060703	4.578535
301.485683	7201.155686	14.766285	-0.060697	4.576090
301.345301	7193.151359	14.771290	-0.060666	4.573629
301.477593	7185.101854	14.776295	-0.060685	4.571153
301.437614	7177.101856	14.781299	-0.060673	4.568691
301.338706	7169.119576	14.786304	-0.060649	4.566232
301.182748	7161.119567	14.791309	-0.060615	4.563767
301.338855	7153.077178	14.796314	-0.060639	4.561288
301.363090	7145.159048	14.801319	-0.060638	4.558846
301.183529	7137.150967	14.806323	-0.060599	4.556374
301.243114	7129.110863	14.811328	-0.060605	4.553891
301.278634	7121.082313	14.816333	-0.060607	4.551411
301.140128	7113.066047	14.821338	-0.060576	4.548933
301.151727	7105.097855	14.826343	-0.060572	4.546468
301.117768	7097.084807	14.831347	-0.060561	4.543988
301.115035	7089.102193	14.836352	-0.060555	4.541517
300.977191	7081.128724	14.841357	-0.060524	4.539046
301.115064	7073.086563	14.846362	-0.060545	4.536554
301.186036	7065.123649	14.851367	-0.060553	4.534084
300.993860	7057.052026	14.856371	-0.060512	4.531579
301.120456	7049.080418	14.861376	-0.060530	4.529104
301.040796	7041.115491	14.866381	-0.060510	4.526630
300.798854	7033.070709	14.871386	-0.060460	4.524129
300.912910	7025.126343	14.876391	-0.060476	4.521658
300.975742	7017.064280	14.881395	-0.060482	4.519150
300.905814	7009.132966	14.886400	-0.060464	4.516680
300.842976	7001.084738	14.891405	-0.060447	4.514173
300.631890	6993.019134	14.896410	-0.060403	4.511659
300.678119	6985.037136	14.901415	-0.060406	4.509169
300.510947	6977.052273	14.906419	-0.060370	4.506677
300.549379	6969.030196	14.911424	-0.060372	4.504173
300.711785	6961.104436	14.916429	-0.060397	4.501698
300.555608	6953.031980	14.921434	-0.060362	4.499174
300.439069	6945.109479	14.926439	-0.060335	4.496696
300.617896	6937.043076	14.931443	-0.060363	4.494173
300.682854	6928.987187	14.936448	-0.060370	4.491651
300.493450	6921.036861	14.941453	-0.060330	4.489160
300.525355	6913.008225	14.946458	-0.060331	4.486643
300.423477	6905.051097	14.951463	-0.060306	4.484148
300.288427	6897.102761	14.956467	-0.060276	4.481653
300.307716	6889.041013	14.961472	-0.060274	4.479122
300.300515	6881.107301	14.966477	-0.060268	4.476630
300.203062	6873.001235	14.971482	-0.060244	4.474082
300.256682	6865.041102	14.976487	-0.060249	4.471578
300.241788	6856.985000	14.981491	-0.060241	4.469043
300.342484	6849.025366	14.986496	-0.060255	4.466538
300.175748	6841.020718	14.991501	-0.060218	4.464015
299.910821	6833.053496	14.996506	-0.060164	4.461503
300.065895	6825.044341	15.001511	-0.060188	4.458978
300.055723	6817.023855	15.006515	-0.060180	4.456447
299.948775	6809.003189	15.011520	-0.060155	4.453914
300.143776	6800.986352	15.016525	-0.060186	4.451382
299.998655	6792.966446	15.021530	-0.060154	4.448846
299.696614	6785.048907	15.026535	-0.060093	4.446341
299.811550	6777.032902	15.031539	-0.060109	4.443804
299.874620	6768.992550	15.036544	-0.060115	4.441259
299.861347	6761.057309	15.041549	-0.060108	4.438745
299.555067	6753.040960	15.046554	-0.060045	4.436202
299.827261	6744.982996	15.051559	-0.060091	4.433647
299.683608	6736.940301	15.056563	-0.060059	4.431094
299.584868	6728.954744	15.061568	-0.060035	4.428558
299.608963	6720.972047	15.066573	-0.060035	4.426021
299.455902	6712.974902	15.071578	-0.060001	4.423478
299.396710	6704.955532	15.076583	-0.059985	4.420927
299.354966	6697.003320	15.081587	-0.059972	4.418396
299.375482	6688.957727	15.086592	-0.059970	4.415833
299.282084	6680.965561	15.091597	-0.059948	4.413286
299.267165	6672.923978	15.096602	-0.059940	4.410722
299.556086	6664.967427	15.101607	-0.059988	4.408185
299.082625	6656.923830	15.106611	-0.059895	4.405615
299.208591	6648.975146	15.111616	-0.059913	4.403077
299.421632	6640.983687	15.116621	-0.059948	4.400524
299.335872	6632.994880	15.121626	-0.059926	4.397969
299.181087	6624.996301	15.126631	-0.059892	4.395409
299.041093	6616.978805	15.131635	-0.059861	4.392841
299.211139	6608.898414	15.136640	-0.059887	4.390254
299.251422	6600.961291	15.141645	-0.059890	4.387710
299.052474	6592.908370	15.146650	-0.059847	4.385126
299.262623	6584.987284	15.151655	-0.059881	4.382586
299.035539	6576.919101	15.156659	-0.059834	4.379994
298.975656	6569.029583	15.161664	-0.059818	4.377459
298.976532	6561.003751	15.166669	-0.059812	4.374879
298.935737	6552.937824	15.171674	-0.059800	4.372284
298.906187	6544.929835	15.176679	-0.059789	4.369706
298.759529	6536.982098	15.181683	-0.059756	4.367146
298.612766	6528.937388	15.186688	-0.059724	4.364553
298.692890	6521.069350	15.191693	-0.059734	4.362017
298.569626	6512.957302	15.196698	-0.059705	4.359399
298.842442	6505.013566	15.201703	-0.059751	4.356836
298.699702	6496.956999	15.206707	-0.059719	4.354233
298.565803	6488.852025	15.211712	-0.059689	4.351613
298.764398	6480.886201	15.216717	-0.059721	4.349038
298.626797	6472.888460	15.221722	-0.059690	4.346449
298.370803	6464.928827	15.226727	-0.059637	4.343871
298.301628	6456.947035	15.231731	-0.059619	4.341284
298.533072	6448.959889	15.236736	-0.059657	4.338697
298.604142	6440.991398	15.241741	-0.059665	4.336113
298.479768	6432.897168	15.246746	-0.059636	4.333485
298.525437	6424.903240	15.251751	-0.059640	4.330889
298.570951	6416.923702	15.256755	-0.059643	4.328297
298.595694	6408.942671	15.261760	-0.059642	4.325702
298.548675	6401.008305	15.266765	-0.059628	4.323121
298.155276	6392.972330	15.271770	-0.059550	4.320502
298.262692	6384.979001	15.276775	-0.059565	4.317899
298.250451	6376.898367	15.281779	-0.059557	4.315265
298.275480	6368.903173	15.286784	-0.059557	4.312658
298.256266	6360.913834	15.291789	-0.059548	4.310051
298.038451	6352.891904	15.296794	-0.059502	4.307430
298.006642	6344.923132	15.301799	-0.059491	4.304826
298.031406	6336.958818	15.306803	-0.059490	4.302223
297.834395	6328.861491	15.311808	-0.059448	4.299573
298.057834	6320.975593	15.316813	-0.059485	4.296993
298.012685	6312.895967	15.321818	-0.059471	4.294347
298.077558	6304.916756	15.326823	-0.059478	4.291732
298.011742	6296.888498	15.331827	-0.059460	4.289099
297.792695	6288.904200	15.336832	-0.059415	4.286478
297.889190	6280.947414	15.341837	-0.059427	4.283866
297.710093	6272.874137	15.346842	-0.059389	4.281212
297.718597	6264.944550	15.351847	-0.059385	4.278606
297.799946	6256.928742	15.356851	-0.059395	4.275970
297.667724	6248.891115	15.361856	-0.059365	4.273323
297.699981	6240.874159	15.366861	-0.059366	4.270683
297.660254	6232.862144	15.371866	-0.059353	4.268043
297.634297	6224.875572	15.376871	-0.059343	4.265409
297.588633	6216.890691	15.381875	-0.059330	4.262774
297.575593	6208.858852	15.386880	-0.059322	4.260122
297.518549	6200.906903	15.391885	-0.059306	4.257495
297.327150	6192.905001	15.396890	-0.059265	4.254848
297.304510	6184.898835	15.401895	-0.059256	4.252200
297.483254	6176.848753	15.406899	-0.059284	4.249537
297.504756	6168.873036	15.411904	-0.059283	4.246896
297.296922	6160.911505	15.416909	-0.059239	4.244255
297.349884	6152.899690	15.421914	-0.059243	4.241599
297.415365	6144.903813	15.426919	-0.059250	4.238947
297.375128	6136.947894	15.431923	-0.059238	4.236305
297.285462	6128.899739	15.436928	-0.059216	4.233630
297.416889	6120.872862	15.441933	-0.059235	4.230963
297.112978	6112.868348	15.446938	-0.059173	4.228297
297.234425	6104.900634	15.451943	-0.059190	4.225647
297.031624	6096.938060	15.456947	-0.059148	4.222993
297.014155	6088.861773	15.461952	-0.059139	4.220301
297.190821	6080.933664	15.466957	-0.059167	4.217659
297.269491	6072.897427	15.471962	-0.059176	4.214978
297.213423	6064.943257	15.476967	-0.059161	4.212321
296.996197	6056.887881	15.481971	-0.059115	4.209628
296.883742	6048.921364	15.486976	-0.059089	4.206963
297.028763	6040.932425	15.491981	-0.059110	4.204292
296.911994	6032.940778	15.496986	-0.059084	4.201615
296.759040	6024.973110	15.501991	-0.059050	4.198945
296.878723	6016.910774	15.506995	-0.059067	4.196244
296.740804	6008.861724	15.512000	-0.059036	4.193542
296.716536	6000.796644	15.517005	-0.059026	4.190835
296.459857	5992.838085	15.522010	-0.058973	4.188160
296.528573	5984.846395	15.527015	-0.058981	4.185475
296.549955	5976.904965	15.532019	-0.058980	4.182805
296.489366	5968.865538	15.537024	-0.058963	4.180099
296.462347	5960.920159	15.542029	-0.058953	4.177423
296.430844	5952.886479	15.547034	-0.058942	4.174716
296.312654	5944.919223	15.552039	-0.058914	4.172029
296.260974	5936.879080	15.557043	-0.058900	4.169316
296.342037	5928.870258	15.562048	-0.058909	4.166613
296.401976	5920.871016	15.567053	-0.058915	4.163911
296.302409	5912.882356	15.572058	-0.058892	4.161210
296.205133	5904.905313	15.577063	-0.058868	4.158511
296.203949	5896.921903	15.582067	-0.058863	4.155809
296.232466	5888.835774	15.587072	-0.058863	4.153070
296.281594	5880.863845	15.592077	-0.058867	4.150369
296.025650	5872.845155	15.597082	-0.058814	4.147647
295.979456	5864.824485	15.602087	-0.058800	4.144924
296.136355	5856.900291	15.607091	-0.058824	4.142235
295.911439	5848.841338	15.612096	-0.058777	4.139494
295.976264	5840.920681	15.617101	-0.058784	4.136802
295.981092	5832.858714	15.622106	-0.058780	4.134059
296.006304	5824.871035	15.627111	-0.058779	4.131340
296.152992	5816.877799	15.632115	-0.058801	4.128618
296.097706	5808.827562	15.637120	-0.058786	4.125873
296.122712	5800.898704	15.642125	-0.058785	4.123168
295.985950	5792.893233	15.647130	-0.058754	4.120434
295.810939	5784.917396	15.652135	-0.058717	4.117707
295.684712	5776.881196	15.657139	-0.058688	4.114958
295.709778	5768.822870	15.662144	-0.058687	4.112202
295.545406	5760.839066	15.667149	-0.058652	4.109468
295.605799	5752.844870	15.672154	-0.058658	4.106730
295.578229	5744.847491	15.677159	-0.058647	4.103989
295.476166	5736.868326	15.682163	-0.058623	4.101251
295.534036	5728.876583	15.687168	-0.058629	4.098509
295.570452	5720.906447	15.692173	-0.058630	4.095772
295.501166	5712.873984	15.697178	-0.058612	4.093010
295.208968	5704.853845	15.702183	-0.058552	4.090248
295.343774	5696.886929	15.707187	-0.058572	4.087509
295.385820	5688.842857	15.712192	-0.058575	4.084739
295.414644	5680.923398	15.717197	-0.058575	4.082010
295.311120	5672.897731	15.722202	-0.058551	4.079242
295.299957	5664.943521	15.727207	-0.058543	4.076497
295.365362	5656.902129	15.732211	-0.058550	4.073721
295.116377	5648.863513	15.737216	-0.058499	4.070940
295.140557	5640.908797	15.742221	-0.058498	4.068190
295.045666	5632.893947	15.747226	-0.058475	4.065415
294.938064	5624.955442	15.752231	-0.058450	4.062665
294.895413	5616.910705	15.757235	-0.058437	4.059877
295.028842	5608.925462	15.762240	-0.058456	4.057110
295.038882	5600.923748	15.767245	-0.058453	4.054334
294.966187	5592.914784	15.772250	-0.058434	4.051552
294.803332	5584.901657	15.777255	-0.058399	4.048766
294.917225	5576.929164	15.782259	-0.058415	4.045996
294.959117	5568.914001	15.787264	-0.058417	4.043208
294.964554	5560.917557	15.792269	-0.058413	4.040424
294.952132	5552.956055	15.797274	-0.058405	4.037650
294.830577	5544.909820	15.802279	-0.058378	4.034843
294.624499	5536.850514	15.807283	-0.058334	4.032028
294.565850	5528.803075	15.812288	-0.058318	4.029218
294.668625	5520.900780	15.817293	-0.058332	4.026459
294.421886	5512.856631	15.822298	-0.058281	4.023643
294.527628	5504.877724	15.827303	-0.058295	4.020853
294.617600	5496.913035	15.832307	-0.058307	4.018066
294.553618	5488.884921	15.837312	-0.058289	4.015252
294.545298	5480.911631	15.842317	-0.058283	4.012457
294.336413	5472.830973	15.847322	-0.058238	4.009619
294.377287	5464.912076	15.852327	-0.058241	4.006839
294.287030	5456.890852	15.857331	-0.058219	4.004020
294.179976	5448.930230	15.862336	-0.058194	4.001219
294.340090	5440.940945	15.867341	-0.058218	3.998411
294.125518	5432.898037	15.872346	-0.058173	3.995576
294.072930	5424.885418	15.877351	-0.058158	3.992752
294.147141	5416.865593	15.882355	-0.058167	3.989926
293.875187	5408.870042	15.887360	-0.058111	3.987100
294.096570	5400.883071	15.892365	-0.058147	3.984284
294.024660	5392.911766	15.897370	-0.058128	3.981466
294.011295	5384.920457	15.902375	-0.058121	3.978641
293.898537	5376.928032	15.907379	-0.058094	3.975811
293.996839	5368.889108	15.912384	-0.058107	3.972966
293.973990	5360.882773	15.917389	-0.058098	3.970129
293.832765	5352.894838	15.922394	-0.058066	3.967294
293.791982	5344.885024	15.927399	-0.058054	3.964451
293.992051	5336.984591	15.932403	-0.058086	3.961649
293.817055	5328.952235	15.937408	-0.058048	3.958792
293.721163	5320.976357	15.942413	-0.058025	3.955954
293.694079	5312.945035	15.947418	-0.058015	3.953095
293.861441	5304.905705	15.952423	-0.058040	3.950235
293.828583	5296.922191	15.957427	-0.058029	3.947390
293.582228	5288.903289	15.962432	-0.057978	3.944526
293.663532	5280.967766	15.967437	-0.057988	3.941695
293.528676	5272.948978	15.972442	-0.057958	3.938829
293.554409	5264.932494	15.977447	-0.057957	3.935964
293.504944	5256.963105	15.982451	-0.057943	3.933112
293.461177	5248.945180	15.987456	-0.057929	3.930242
293.306105	5240.998840	15.992461	-0.057895	3.927393
293.357872	5232.924293	15.997466	-0.057900	3.924499
293.413393	5224.974684	16.002471	-0.057905	3.921648
293.296395	5216.981347	16.007475	-0.057878	3.918777
293.252171	5208.981532	16.012480	-0.057864	3.915902
293.378255	5201.006686	16.017485	-0.057883	3.913037
293.130145	5192.950147	16.022490	-0.057831	3.910134
293.106167	5184.944497	16.027495	-0.057822	3.907251
293.091887	5176.945137	16.032499	-0.057814	3.904369
292.988911	5168.987460	16.037504	-0.057789	3.901497
292.864142	5161.013476	16.042509	-0.057761	3.898618
293.018467	5152.971216	16.047514	-0.057784	3.895716
293.027849	5144.955450	16.052519	-0.057781	3.892820
293.134229	5136.936228	16.057523	-0.057795	3.889922
292.923064	5128.968191	16.062528	-0.057751	3.887034
292.913934	5120.964431	16.067533	-0.057744	3.884135
292.791223	5112.986484	16.072538	-0.057716	3.881241
292.617260	5105.018146	16.077543	-0.057678	3.878347
292.731559	5097.012000	16.082547	-0.057694	3.875443
292.650877	5088.769750	16.087552	-0.057674	3.872447
292.509727	5080.790413	16.092557	-0.057643	3.869543
292.616699	5072.879158	16.097562	-0.057657	3.866667
292.585400	5064.884423	16.102567	-0.057646	3.863755
292.585861	5056.954808	16.107571	-0.057641	3.860866
292.484685	5048.946846	16.112576	-0.057617	3.857944
292.814761	5040.968313	16.117581	-0.057673	3.855039
292.517041	5032.946572	16.122586	-0.057613	3.852103
292.482028	5024.965198	16.127591	-0.057601	3.849185
292.596238	5016.954299	16.132595	-0.057617	3.846257
292.549806	5008.964388	16.137600	-0.057603	3.843332
292.413534	5001.035878	16.142605	-0.057573	3.840425
292.390473	4993.022803	16.147610	-0.057563	3.837486
292.422551	4985.019578	16.152615	-0.057564	3.834551
292.255314	4977.015898	16.157619	-0.057527	3.831609
292.123241	4968.973135	16.162624	-0.057498	3.828651
292.336166	4960.992535	16.167629	-0.057532	3.825720
292.149433	4953.034864	16.172634	-0.057492	3.822788
291.906622	4945.066265	16.177639	-0.057442	3.819848
292.109437	4937.069810	16.182643	-0.057474	3.816905
292.154484	4929.014098	16.187648	-0.057477	3.813934
291.981006	4921.011964	16.192653	-0.057440	3.810976
291.928095	4913.031927	16.197658	-0.057425	3.808027
291.929418	4905.043122	16.202663	-0.057420	3.805073
291.797245	4897.096168	16.207667	-0.057390	3.802130
291.635100	4889.089770	16.212672	-0.057355	3.799161
291.737341	4881.107823	16.217677	-0.057368	3.796205
291.823268	4873.071595	16.222682	-0.057379	3.793227
291.688058	4865.004309	16.227687	-0.057349	3.790229
291.718506	4857.040312	16.232691	-0.057349	3.787272
291.704017	4849.033166	16.237696	-0.057341	3.784294
291.607940	4841.117739	16.242701	-0.057318	3.781347
291.476569	4833.069008	16.247706	-0.057289	3.778347
291.533155	4825.069846	16.252711	-0.057294	3.775368
291.666013	4817.038063	16.257715	-0.057313	3.772375
291.545967	4809.039639	16.262720	-0.057286	3.769387
291.681088	4801.102278	16.267725	-0.057306	3.766425
291.540673	4793.062697	16.272730	-0.057274	3.763417
291.438612	4785.083152	16.277735	-0.057250	3.760429
291.448812	4777.118111	16.282739	-0.057247	3.757447
291.408244	4769.061752	16.287744	-0.057234	3.754427
291.268536	4761.097077	16.292749	-0.057203	3.751437
291.395062	4753.048320	16.297754	-0.057221	3.748418
291.235783	4745.068627	16.302759	-0.057186	3.745417
291.351040	4737.103189	16.307763	-0.057203	3.742425
291.244838	4729.094062	16.312768	-0.057178	3.739410
291.444087	4721.143558	16.317773	-0.057209	3.736421
291.277024	4713.082439	16.322778	-0.057173	3.733379
291.048057	4705.095591	16.327783	-0.057125	3.730361
290.990123	4697.128458	16.332787	-0.057109	3.727352
291.076208	4689.069422	16.337792	-0.057120	3.724310
291.133664	4681.150831	16.342797	-0.057126	3.721318
290.964490	4673.161527	16.347802	-0.057089	3.718291
291.094071	4665.160482	16.352807	-0.057108	3.715264
291.059775	4657.108924	16.357811	-0.057096	3.712211
290.914087	4649.063789	16.362816	-0.057064	3.709156
291.023451	4641.097637	16.367821	-0.057079	3.706135
290.964304	4633.110267	16.372826	-0.057063	3.703099
290.669859	4625.133301	16.377831	-0.057003	3.700058
290.803758	4617.185914	16.382835	-0.057022	3.697037
290.741385	4609.161954	16.387840	-0.057006	3.693979
290.632309	4601.173116	16.392845	-0.056980	3.690931
290.388923	4593.196503	16.397850	-0.056930	3.687882
290.486007	4585.146087	16.402855	-0.056942	3.684810
290.568891	4577.230683	16.407859	-0.056953	3.681788
290.481667	4569.226157	16.412864	-0.056931	3.678724
290.450182	4561.231967	16.417869	-0.056920	3.675663
290.590588	4553.199575	16.422874	-0.056941	3.672590
290.271657	4545.182652	16.427879	-0.056876	3.669508
290.443048	4537.212041	16.432883	-0.056903	3.666453
290.469210	4529.200098	16.437888	-0.056903	3.663377
290.533111	4521.214249	16.442893	-0.056909	3.660309
290.205407	4513.255938	16.447898	-0.056843	3.657239
290.118130	4505.228952	16.452903	-0.056822	3.654146
290.382216	4497.219679	16.457907	-0.056866	3.651066
290.040288	4489.230967	16.462912	-0.056797	3.647976
290.008081	4481.226335	16.467917	-0.056786	3.644885
289.996387	4473.273951	16.472922	-0.056778	3.641813
290.048574	4465.266584	16.477927	-0.056783	3.638718
289.980381	4457.266272	16.482931	-0.056765	3.635620
290.101602	4449.198451	16.487936	-0.056782	3.632498
289.954365	4441.236680	16.492941	-0.056749	3.629408
289.858915	4433.246784	16.497946	-0.056727	3.626305
289.885839	4425.234326	16.502951	-0.056726	3.623194
289.998396	4417.246828	16.507955	-0.056742	3.620093
289.719365	4409.289644	16.512960	-0.056685	3.616990
289.593360	4401.309397	16.517965	-0.056656	3.613880
289.750020	4393.266452	16.522970	-0.056680	3.610750
289.706024	4385.283844	16.527975	-0.056667	3.607635
289.510120	4377.311756	16.532979	-0.056625	3.604518
289.438492	4369.327418	16.537984	-0.056607	3.601397
289.655931	4361.329385	16.542989	-0.056642	3.598275
289.457349	4353.344086	16.547994	-0.056600	3.595144
289.458642	4345.311645	16.552999	-0.056595	3.591998
289.455008	4337.331973	16.558003	-0.056589	3.588869
289.431649	4329.321722	16.563008	-0.056579	3.585726
289.360627	4321.388709	16.568013	-0.056561	3.582608
289.145720	4313.366706	16.573018	-0.056515	3.579449
289.100524	4305.390297	16.578023	-0.056502	3.576309
289.297151	4297.373150	16.583027	-0.056533	3.573158
289.182355	4289.334321	16.588032	-0.056507	3.569986
289.176118	4281.372253	16.593037	-0.056500	3.566845
289.159910	4273.369727	16.598042	-0.056492	3.563685
289.041495	4265.384222	16.603047	-0.056465	3.560526
289.169298	4257.427099	16.608051	-0.056483	3.557382
289.073698	4249.405239	16.613056	-0.056460	3.554204
288.937439	4241.323535	16.618061	-0.056430	3.550997
288.970657	4233.353804	16.623066	-0.056431	3.547838
288.957277	4225.329396	16.628071	-0.056423	3.544652
288.831928	4217.401504	16.633075	-0.056394	3.541498
288.748625	4209.384193	16.638080	-0.056374	3.538308
288.871570	4201.408016	16.643085	-0.056391	3.535137
288.527827	4193.451471	16.648090	-0.056322	3.531957
288.553104	4185.407794	16.653095	-0.056322	3.528750
288.537620	4177.437849	16.658099	-0.056314	3.525569
288.558598	4169.447339	16.663104	-0.056312	3.522377
288.794160	4161.428964	16.668109	-0.056351	3.519179
288.475053	4153.469557	16.673114	-0.056286	3.515984
288.519458	4145.447594	16.678119	-0.056289	3.512772
288.567009	4137.439717	16.683123	-0.056293	3.509562
288.524190	4129.457776	16.688128	-0.056280	3.506358
288.503537	4121.482999	16.693133	-0.056271	3.503154
288.529100	4113.484785	16.698138	-0.056270	3.499940
288.249457	4105.537772	16.703143	-0.056213	3.496733
288.413996	4097.526421	16.708147	-0.056238	3.493511
288.313176	4089.484267	16.713152	-0.056214	3.490266
288.338966	4081.541047	16.718157	-0.056214	3.487062
288.318709	4073.557740	16.723162	-0.056205	3.483837
288.383877	4065.546564	16.728167	-0.056212	3.480600
288.309147	4057.602424	16.733171	-0.056193	3.477383
288.321376	4049.559415	16.738176	-0.056190	3.474126
288.258208	4041.522992	16.743181	-0.056173	3.470866
288.215286	4033.555605	16.748186	-0.056160	3.467631
288.055957	4025.538098	16.753191	-0.056125	3.464370
288.105121	4017.608303	16.758195	-0.056129	3.461148
287.893910	4009.608537	16.763200	-0.056084	3.457886
287.872762	4001.602721	16.768205	-0.056075	3.454624
288.004682	3993.614379	16.773210	-0.056094	3.451371
287.957541	3985.587523	16.778215	-0.056080	3.448094
288.059755	3977.598284	16.783219	-0.056094	3.444834
287.753655	3969.620607	16.788224	-0.056032	3.441562
287.875185	3961.644185	16.793229	-0.056049	3.438302
287.678391	3953.656980	16.798234	-0.056008	3.435024
287.706706	3945.628706	16.803239	-0.056008	3.431733
287.928698	3937.617392	16.808243	-0.056044	3.428452
287.722163	3929.613801	16.813248	-0.056000	3.425157
287.767978	3921.660282	16.818253	-0.056003	3.421888
287.853602	3913.665584	16.823258	-0.056014	3.418600
287.577424	3905.664453	16.828263	-0.055957	3.415295
287.557517	3897.700713	16.833267	-0.055949	3.412010
287.415988	3889.687458	16.838272	-0.055917	3.408697
287.494646	3881.706821	16.843277	-0.055926	3.405402
287.323045	3873.744902	16.848282	-0.055889	3.402103
287.247761	3865.749590	16.853287	-0.055870	3.398790
287.540200	3857.775786	16.858291	-0.055919	3.395496
287.326590	3849.675230	16.863296	-0.055874	3.392128
287.256704	3841.702261	16.868301	-0.055856	3.388815
287.212608	3833.695914	16.873306	-0.055843	3.385486
287.233441	3825.739240	16.878311	-0.055841	3.382176
287.256986	3817.778880	16.883315	-0.055840	3.378862
287.045521	3809.784121	16.888320	-0.055796	3.375521
286.994947	3801.802402	16.893325	-0.055781	3.372189
287.182202	3793.790413	16.898330	-0.055811	3.368849
286.978009	3785.783882	16.903335	-0.055768	3.365494
287.125841	3777.845529	16.908339	-0.055790	3.362177
287.057725	3769.830676	16.913344	-0.055772	3.358817
286.828313	3761.851139	16.918349	-0.055724	3.355462
286.836094	3753.843650	16.923354	-0.055720	3.352101
286.807412	3745.834718	16.928359	-0.055710	3.348735
286.907609	3737.860539	16.933363	-0.055723	3.345384
286.817414	3729.866352	16.938368	-0.055701	3.342015
286.896410	3721.864087	16.943373	-0.055711	3.338645
286.845185	3713.866421	16.948378	-0.055696	3.335269
286.722529	3705.880162	16.953383	-0.055668	3.331891
286.764418	3697.903166	16.958387	-0.055671	3.328521
286.738964	3689.870092	16.963392	-0.055661	3.325120
286.663643	3681.945392	16.968397	-0.055641	3.321760
286.541838	3673.970297	16.973402	-0.055613	3.318374
286.450690	3665.956594	16.978407	-0.055591	3.314969
286.405601	3657.964722	16.983411	-0.055578	3.311571
286.204934	3649.953792	16.988416	-0.055535	3.308156
286.497566	3641.932318	16.993421	-0.055584	3.304751
286.468395	3633.980573	16.998426	-0.055574	3.301361
286.416148	3625.975450	17.003431	-0.055559	3.297943
286.259254	3618.040613	17.008435	-0.055524	3.294548
286.081038	3610.022532	17.013440	-0.055486	3.291113
286.092583	3602.032319	17.018445	-0.055483	3.287693
286.139040	3594.015232	17.023450	-0.055486	3.284260
285.941182	3586.070016	17.028455	-0.055444	3.280845
286.114986	3578.098848	17.033459	-0.055471	3.277429
285.998116	3570.061332	17.038464	-0.055444	3.273970
285.858133	3562.062752	17.043469	-0.055413	3.270523
286.154317	3554.067044	17.048474	-0.055463	3.267090
285.936995	3546.076482	17.053479	-0.055417	3.263636
285.858473	3538.123013	17.058483	-0.055398	3.260200
285.810868	3530.146253	17.063488	-0.055384	3.256752
285.699386	3522.126120	17.068493	-0.055358	3.253278
285.617435	3514.104689	17.073498	-0.055337	3.249802
285.633867	3506.140407	17.078503	-0.055335	3.246350
285.674100	3498.150036	17.083507	-0.055337	3.242884
285.508687	3490.179317	17.088512	-0.055301	3.239415
285.487820	3482.220322	17.093517	-0.055292	3.235953
285.685984	3474.145578	17.098522	-0.055324	3.232446
285.380450	3466.155756	17.103527	-0.055262	3.228951
285.496238	3458.158314	17.108531	-0.055278	3.225467
285.397417	3450.195956	17.113536	-0.055254	3.221985
285.547784	3442.206778	17.118541	-0.055277	3.218498
285.298300	3434.250894	17.123546	-0.055226	3.215006
285.295639	3426.232852	17.128551	-0.055220	3.211492
285.351727	3418.233700	17.133555	-0.055225	3.207985
285.327154	3410.240942	17.138560	-0.055215	3.204474
285.158359	3402.323131	17.143565	-0.055179	3.200987
285.392162	3394.305665	17.148570	-0.055217	3.197468
285.082208	3386.335841	17.153575	-0.055154	3.193943
285.071361	3378.328801	17.158579	-0.055147	3.190411
284.990799	3370.329516	17.163584	-0.055127	3.186875
284.969218	3362.357512	17.168589	-0.055117	3.183350
284.817055	3354.388530	17.173594	-0.055084	3.179817
284.743173	3346.366741	17.178599	-0.055065	3.176260
284.865447	3338.380131	17.183603	-0.055082	3.172723
284.718894	3330.387526	17.188608	-0.055050	3.169167
284.646791	3322.403794	17.193613	-0.055031	3.165615
284.706894	3314.440106	17.198618	-0.055037	3.162074
284.612224	3306.437293	17.203623	-0.055014	3.158504
284.798216	3298.456881	17.208627	-0.055044	3.154952
284.734828	3290.446058	17.213632	-0.055027	3.151372
284.710368	3282.443367	17.218637	-0.055017	3.147794
284.439344	3274.473892	17.223642	-0.054961	3.144215
284.625668	3266.466053	17.228647	-0.054991	3.140635
284.546011	3258.522568	17.233651	-0.054971	3.137068
284.478328	3250.518896	17.238656	-0.054953	3.133470
284.377110	3242.522898	17.243661	-0.054929	3.129871
284.538869	3234.549706	17.248666	-0.054954	3.126289
284.426280	3226.561471	17.253671	-0.054928	3.122684
284.376119	3218.596388	17.258675	-0.054913	3.119088
284.342291	3210.613340	17.263680	-0.054902	3.115480
284.226066	3202.608426	17.268685	-0.054875	3.111855
284.199323	3194.629482	17.273690	-0.054865	3.108241
283.867718	3186.618001	17.278695	-0.054798	3.104595
284.083022	3178.676199	17.283699	-0.054832	3.101001
284.039188	3170.677455	17.288704	-0.054819	3.097364
283.988682	3162.653817	17.293709	-0.054804	3.093712
284.059347	3154.666538	17.298714	-0.054812	3.090078
283.901695	3146.686325	17.303719	-0.054778	3.086432
283.982582	3138.720233	17.308723	-0.054788	3.082799
283.788583	3130.742843	17.313728	-0.054746	3.079144
284.041714	3122.749458	17.318733	-0.054788	3.075499
283.777729	3114.707633	17.323738	-0.054734	3.071802
283.668871	3106.708811	17.328743	-0.054708	3.068128
283.847518	3098.701176	17.333747	-0.054736	3.064459
283.855301	3090.768005	17.338752	-0.054733	3.060812
283.746150	3082.808134	17.343757	-0.054707	3.057143
283.785202	3074.825752	17.348762	-0.054709	3.053466
283.773315	3066.801405	17.353767	-0.054702	3.049762
283.705925	3058.863438	17.358771	-0.054684	3.046092
283.543628	3050.870666	17.363776	-0.054649	3.042387
283.443800	3042.904166	17.368781	-0.054625	3.038693
283.478265	3034.937541	17.373786	-0.054626	3.035000
283.287386	3026.921977	17.378791	-0.054585	3.031270
283.443479	3018.936036	17.383795	-0.054609	3.027565
283.307323	3010.952005	17.388800	-0.054579	3.023843
283.232170	3002.956784	17.393805	-0.054559	3.020114
283.272812	2995.006859	17.398810	-0.054562	3.016407
283.240007	2986.978196	17.403815	-0.054550	3.012655
283.371387	2978.979690	17.408819	-0.054570	3.008920
283.171896	2971.014490	17.413824	-0.054527	3.005180
283.246967	2963.055692	17.418829	-0.054536	3.001452
283.167766	2955.101748	17.423834	-0.054516	2.997714
282.971002	2947.105803	17.428839	-0.054474	2.993946
282.887067	2939.104772	17.433843	-0.054453	2.990176
283.059625	2931.092634	17.438848	-0.054480	2.986409
282.972030	2923.104270	17.443853	-0.054459	2.982636
282.939426	2915.160495	17.448858	-0.054448	2.978881
283.105725	2907.132992	17.453863	-0.054473	2.975092
282.935931	2899.178538	17.458867	-0.054437	2.971316
282.888075	2891.183736	17.463872	-0.054422	2.967522
282.897422	2883.200281	17.468877	-0.054419	2.963732
283.022018	2875.246156	17.473882	-0.054437	2.959956
282.791592	2867.294436	17.478887	-0.054389	2.956159
282.614831	2859.294908	17.483891	-0.054351	2.952337
282.647928	2851.292326	17.488896	-0.054352	2.948519
282.799055	2843.265783	17.493901	-0.054375	2.944691
282.565893	2835.362306	17.498906	-0.054326	2.940897
282.386255	2827.361114	17.503911	-0.054287	2.937053
282.449059	2819.351929	17.508915	-0.054294	2.933214
282.393635	2811.348544	17.513920	-0.054278	2.929366
282.305844	2803.408529	17.518925	-0.054257	2.925542
282.357764	2795.432578	17.523930	-0.054261	2.921703
282.094815	2787.461462	17.528935	-0.054207	2.917844
282.190849	2779.479088	17.533939	-0.054220	2.913994
282.265347	2771.377325	17.538944	-0.054228	2.910080
282.280705	2763.397951	17.543949	-0.054226	2.906217
282.178792	2755.488440	17.548954	-0.054202	2.902376
282.164122	2747.495638	17.553959	-0.054194	2.898495
282.221019	2739.519747	17.558963	-0.054199	2.894620
281.811239	2731.575486	17.563968	-0.054118	2.890730
281.964703	2723.539903	17.568973	-0.054141	2.886821
282.057921	2715.598519	17.573978	-0.054153	2.882950
281.993765	2707.612531	17.578983	-0.054136	2.879042
282.035962	2699.659964	17.583987	-0.054139	2.875152
281.926679	2691.640238	17.588992	-0.054113	2.871215
281.957257	2683.654041	17.593997	-0.054114	2.867297
281.860326	2675.698131	17.599002	-0.054090	2.863382
281.790321	2667.713996	17.604007	-0.054072	2.859448
281.704920	2659.772372	17.609011	-0.054051	2.855529
281.695834	2651.763550	17.614016	-0.054044	2.851576
281.521528	2643.795870	17.619021	-0.054007	2.847629
281.410165	2635.839142	17.624026	-0.053981	2.843685
281.485613	2627.825120	17.629031	-0.053989	2.839717
281.494395	2619.898350	17.634035	-0.053986	2.835784
281.482411	2611.871937	17.639040	-0.053978	2.831794
281.389764	2603.867288	17.644045	-0.053956	2.827805
281.449057	2595.887939	17.649050	-0.053962	2.823832
281.478071	2587.899497	17.654055	-0.053962	2.819847
281.610325	2579.935476	17.659059	-0.053981	2.815874
281.253033	2571.980192	17.664064	-0.053910	2.811872
280.972866	2564.025698	17.669069	-0.053852	2.807869
281.205036	2556.010672	17.674074	-0.053890	2.803859
280.977659	2548.071143	17.679079	-0.053843	2.799855
280.972327	2540.112492	17.684083	-0.053837	2.795849
280.732123	2532.102686	17.689088	-0.053787	2.791797
280.750060	2524.097591	17.694093	-0.053785	2.787757
280.848020	2516.118867	17.699098	-0.053798	2.783729
280.431098	2508.194249	17.704103	-0.053715	2.779692
280.756075	2500.183278	17.709107	-0.053770	2.775650
280.613912	2492.208800	17.714112	-0.053739	2.771592
280.751227	2484.198699	17.719117	-0.053759	2.767527
280.639064	2476.253379	17.724122	-0.053733	2.763474
280.657742	2468.276300	17.729127	-0.053731	2.759406
280.673306	2460.343097	17.734131	-0.053729	2.755355
280.580775	2452.267769	17.739136	-0.053706	2.751219
280.512278	2444.287059	17.744141	-0.053688	2.747126
280.337932	2436.353267	17.749146	-0.053651	2.743045
280.318741	2428.357182	17.754151	-0.053642	2.738935
280.413405	2420.384484	17.759155	-0.053654	2.734838
280.318407	2412.415298	17.764160	-0.053632	2.730725
280.266257	2404.442202	17.769165	-0.053617	2.726607
280.449473	2396.476714	17.774170	-0.053646	2.722501
280.227713	2388.518973	17.779175	-0.053599	2.718367
280.313048	2380.547035	17.784179	-0.053610	2.714239
280.279068	2372.532353	17.789184	-0.053598	2.710075
280.313970	2364.560747	17.794189	-0.053600	2.705931
280.229131	2356.630663	17.799194	-0.053579	2.701795
279.962086	2348.654529	17.804199	-0.053524	2.697617
280.186722	2340.666370	17.809203	-0.053560	2.693457
280.062400	2332.691939	17.814208	-0.053532	2.689276
279.947985	2324.716283	17.819213	-0.053505	2.685089
279.963437	2316.777842	17.824218	-0.053503	2.680922
279.901835	2308.810626	17.829223	-0.053486	2.676729
279.953396	2300.794811	17.834227	-0.053491	2.672512
279.850075	2292.800968	17.839232	-0.053466	2.668289
279.755576	2284.816402	17.844237	-0.053444	2.664065
279.788193	2276.876227	17.849242	-0.053444	2.659866
279.619852	2268.926004	17.854247	-0.053408	2.655642
279.732146	2260.923658	17.859251	-0.053424	2.651401
279.486463	2252.974942	17.864256	-0.053373	2.647159
279.545170	2244.990941	17.869261	-0.053378	2.642912
279.478933	2237.052923	17.874266	-0.053361	2.638674
279.507701	2229.044765	17.879271	-0.053361	2.634397
279.474273	2221.059586	17.884275	-0.053350	2.630123
279.436678	2213.089665	17.889280	-0.053337	2.625848
279.411392	2205.128603	17.894285	-0.053327	2.621573
279.499135	2197.179601	17.899290	-0.053339	2.617305
279.265617	2189.205440	17.904295	-0.053290	2.612994
279.197957	2181.225133	17.909299	-0.053272	2.608685
279.419848	2173.235316	17.914304	-0.053308	2.604382
278.986268	2165.316872	17.919309	-0.053222	2.600067
279.136139	2157.357163	17.924314	-0.053245	2.595761
279.067680	2149.200625	17.929319	-0.053227	2.591327
278.966275	2141.250569	17.934323	-0.053203	2.586995
278.751402	2133.331542	17.939328	-0.053158	2.582665
278.818841	2125.367621	17.944333	-0.053165	2.578323
278.856642	2117.421084	17.949338	-0.053167	2.573981
278.709873	2109.437696	17.954343	-0.053134	2.569598
278.796033	2101.477017	17.959347	-0.053145	2.565237
278.809695	2093.540680	17.964352	-0.053143	2.560876
278.524531	2085.606913	17.969357	-0.053084	2.556489
278.776476	2077.608144	17.974362	-0.053126	2.552096
278.681869	2069.616984	17.979367	-0.053103	2.547675
278.510582	2061.685005	17.984371	-0.053066	2.543273
278.391494	2053.742204	17.989376	-0.053039	2.538862
278.626436	2045.736134	17.994381	-0.053077	2.534433
278.822815	2037.744627	17.999386	-0.053109	2.530002
278.473558	2029.821634	18.004391	-0.053038	2.525562
278.523054	2021.864523	18.009395	-0.053042	2.521124
278.424857	2013.926101	18.014400	-0.053019	2.516678
278.157963	2005.936840	18.019405	-0.052964	2.512183
278.241827	1997.951110	18.024410	-0.052974	2.507707
278.194633	1989.968994	18.029415	-0.052960	2.503216
278.035754	1982.032524	18.034419	-0.052926	2.498735
278.181407	1974.065239	18.039424	-0.052948	2.494250
278.158005	1966.067287	18.044429	-0.052938	2.489727
278.091548	1958.132419	18.049434	-0.052921	2.485229
277.681797	1950.224882	18.054439	-0.052839	2.480713
277.804995	1942.243526	18.059443	-0.052857	2.476186
278.004414	1934.229512	18.064448	-0.052889	2.471638
277.701442	1926.286030	18.069453	-0.052827	2.467084
277.777964	1918.316866	18.074458	-0.052836	2.462535
277.587083	1910.376898	18.079463	-0.052795	2.457975
277.599298	1902.412411	18.084467	-0.052793	2.453407
277.430885	1894.445446	18.089472	-0.052756	2.448816
277.311584	1886.488426	18.094477	-0.052729	2.444226
277.604679	1878.514365	18.099482	-0.052778	2.439648
277.487246	1870.570280	18.104487	-0.052751	2.435048
277.585699	1862.510457	18.109491	-0.052764	2.430389
277.555907	1854.556881	18.114496	-0.052753	2.425772
277.254097	1846.640751	18.119501	-0.052692	2.421148
277.329310	1838.701237	18.124506	-0.052701	2.416530
277.325493	1830.706610	18.129511	-0.052695	2.411865
277.299826	1822.749287	18.134515	-0.052685	2.407211
277.299115	1814.795521	18.139520	-0.052679	2.402552
277.290210	1806.854547	18.144525	-0.052673	2.397891
277.383013	1798.897141	18.149530	-0.052685	2.393219
277.283972	1790.915461	18.154535	-0.052661	2.388508
277.434871	1782.938856	18.159539	-0.052684	2.383811
277.212556	1775.042638	18.164544	-0.052637	2.379123
276.961439	1767.104151	18.169549	-0.052585	2.374398
276.837596	1759.142723	18.174554	-0.052557	2.369660
276.927066	1751.164390	18.179559	-0.052569	2.364919
276.928920	1743.226085	18.184563	-0.052564	2.360186
276.801273	1735.296113	18.189568	-0.052535	2.355438
276.806774	1727.281377	18.194573	-0.052531	2.350641
276.743958	1719.323949	18.199578	-0.052514	2.345862
276.517127	1711.385540	18.204583	-0.052466	2.341071
276.483199	1703.438373	18.209587	-0.052455	2.336282
276.427031	1695.483152	18.214592	-0.052439	2.331475
276.292999	1687.513452	18.219597	-0.052409	2.326644
276.458688	1679.562755	18.224602	-0.052435	2.321839
276.504525	1671.603162	18.229607	-0.052438	2.317008
276.614244	1663.632947	18.234611	-0.052453	2.312166
276.331589	1655.700834	18.239616	-0.052395	2.307305
276.363891	1647.738364	18.244621	-0.052396	2.302441
276.360549	1639.802670	18.249626	-0.052391	2.297580
276.241999	1631.855645	18.254631	-0.052363	2.292692
276.068485	1623.916216	18.259635	-0.052326	2.287794
276.072355	1615.956038	18.264640	-0.052321	2.282888
276.146208	1608.001027	18.269645	-0.052330	2.277980
276.238042	1600.020816	18.274650	-0.052342	2.273047
276.052128	1592.023915	18.279655	-0.052302	2.268069
276.032548	1584.086829	18.284659	-0.052293	2.263132
275.890568	1576.179798	18.289664	-0.052261	2.258193
275.979554	1568.190139	18.294669	-0.052273	2.253211
275.976217	1560.245374	18.299674	-0.052267	2.248238
275.889174	1552.308715	18.304679	-0.052246	2.243251
275.590269	1544.423287	18.309683	-0.052185	2.238268
275.694351	1536.447079	18.314688	-0.052199	2.233251
275.707813	1528.470774	18.319693	-0.052196	2.228215
275.679497	1520.544445	18.324698	-0.052186	2.223195
275.550011	1512.615811	18.329703	-0.052157	2.218154
275.521481	1504.660683	18.334707	-0.052146	2.213093
275.599696	1496.694545	18.339712	-0.052155	2.208023
275.442391	1488.772253	18.344717	-0.052121	2.202949
275.376138	1480.861309	18.349722	-0.052104	2.197878
275.287602	1472.902313	18.354727	-0.052082	2.192762
275.381107	1464.894003	18.359731	-0.052094	2.187619
275.335582	1456.974197	18.364736	-0.052080	2.182509
275.221136	1449.037378	18.369741	-0.052054	2.177369
275.050992	1441.123186	18.374746	-0.052017	2.172227
275.109079	1433.144228	18.379751	-0.052023	2.167051
275.142394	1425.206726	18.384755	-0.052024	2.161888
275.331092	1417.269087	18.389760	-0.052054	2.156727
274.932878	1409.358793	18.394765	-0.051974	2.151516
275.075122	1401.384928	18.399770	-0.051996	2.146302
275.048771	1393.443789	18.404775	-0.051986	2.141080
274.858553	1385.553805	18.409779	-0.051945	2.135864
274.906065	1377.594543	18.414784	-0.051949	2.130612
274.805192	1369.649579	18.419789	-0.051925	2.125343
274.851849	1361.725214	18.424794	-0.051928	2.120088
274.767285	1353.798824	18.429799	-0.051907	2.114806
274.765086	1345.768433	18.434803	-0.051902	2.109449
274.699059	1337.860435	18.439808	-0.051884	2.104154
274.509322	1329.945163	18.444813	-0.051844	2.098829
274.594185	1322.018418	18.449818	-0.051854	2.093510
274.560902	1314.066413	18.454823	-0.051843	2.088148
274.457145	1306.152231	18.459827	-0.051818	2.082792
274.578741	1298.216927	18.464832	-0.051836	2.077429
274.419087	1290.277091	18.469837	-0.051801	2.072022
274.330416	1282.363983	18.474842	-0.051779	2.066625
274.210673	1274.436162	18.479847	-0.051752	2.061201
274.273025	1266.503779	18.484851	-0.051758	2.055779
274.178059	1258.585312	18.489856	-0.051735	2.050335
274.123533	1250.632148	18.494861	-0.051720	2.044857
274.343559	1242.711060	18.499866	-0.051756	2.039415
274.254934	1234.777212	18.504871	-0.051734	2.033917
274.054387	1226.844482	18.509875	-0.051692	2.028394
273.951156	1218.937071	18.514880	-0.051667	2.022884
273.849762	1211.013889	18.519885	-0.051643	2.017347
274.011051	1203.070339	18.524890	-0.051668	2.011809
273.959958	1195.131934	18.529895	-0.051653	2.006236
273.699661	1187.249041	18.534899	-0.051600	2.000665
273.668476	1179.341466	18.539904	-0.051589	1.995086
273.515476	1171.401813	18.544909	-0.051555	1.989455
273.715648	1163.449554	18.549914	-0.051587	1.983836
273.687855	1155.538472	18.554919	-0.051577	1.978206
273.567777	1147.631543	18.559923	-0.051549	1.972554
273.422447	1139.723443	18.564928	-0.051517	1.966882
273.359473	1131.811588	18.569933	-0.051500	1.961199
273.377969	1123.908754	18.574938	-0.051499	1.955516
273.156318	1115.949934	18.579943	-0.051452	1.949749
273.153462	1108.017505	18.584947	-0.051446	1.944008
273.179559	1100.106490	18.589952	-0.051446	1.938268
273.134314	1092.166432	18.594957	-0.051432	1.932483
272.984190	1084.281117	18.599962	-0.051399	1.926709
272.850849	1076.375929	18.604967	-0.051369	1.920904
272.934909	1068.461233	18.609971	-0.051380	1.915099
272.763006	1060.548231	18.614976	-0.051343	1.909250
272.786224	1052.606422	18.619981	-0.051342	1.903382
272.966477	1044.701392	18.624986	-0.051370	1.897542
272.852524	1036.788481	18.629991	-0.051344	1.891644
272.741386	1028.879617	18.634995	-0.051318	1.885731
272.810690	1020.974191	18.640000	-0.051326	1.879823
272.636461	1013.097008	18.645005	-0.051288	1.873890
272.685342	1005.158279	18.650010	-0.051292	1.867916
272.529422	997.259653	18.655015	-0.051258	1.861931
272.467247	989.366221	18.660019	-0.051241	1.855941
272.382420	981.462615	18.665024	-0.051220	1.849921
272.282794	973.558238	18.670029	-0.051197	1.843879
272.344498	965.668687	18.675034	-0.051203	1.837847
272.257129	957.757645	18.680039	-0.051181	1.831761
272.173847	949.847020	18.685043	-0.051161	1.825656
272.219709	941.962538	18.690048	-0.051164	1.819566
272.219002	934.059722	18.695053	-0.051159	1.813436
272.157349	926.159368	18.700058	-0.051142	1.807280
271.990745	918.281831	18.705063	-0.051106	1.801107
272.114488	910.384245	18.710067	-0.051124	1.794933
272.033296	902.445188	18.715072	-0.051104	1.788680
271.823122	894.567971	18.720077	-0.051059	1.782438
271.935550	886.677393	18.725082	-0.051075	1.776204
271.707894	878.802405	18.730087	-0.051028	1.769917
271.590661	870.928387	18.735091	-0.051001	1.763623
271.567593	863.059477	18.740096	-0.050991	1.757322
271.499971	855.150656	18.745101	-0.050974	1.750960
271.419820	847.265786	18.750106	-0.050953	1.744593
271.500098	839.376323	18.755111	-0.050963	1.738219
271.578940	831.478099	18.760115	-0.050973	1.731815
271.562780	823.596547	18.765120	-0.050965	1.725388
271.240100	815.774792	18.770125	-0.050899	1.718947
271.255707	807.896749	18.775130	-0.050897	1.712478
271.075578	800.013474	18.780135	-0.050859	1.705956
271.270941	792.102929	18.785139	-0.050890	1.699435
271.275067	784.233949	18.790144	-0.050885	1.692898
271.037366	776.369652	18.795149	-0.050836	1.686308
270.985484	768.522115	18.800154	-0.050821	1.679731
270.902401	760.659099	18.805159	-0.050801	1.673110
270.902640	752.763239	18.810163	-0.050795	1.666447
270.930712	744.909000	18.815168	-0.050796	1.659796
270.654649	737.069342	18.820173	-0.050739	1.653090
270.670083	729.188298	18.825178	-0.050737	1.646360
270.697949	721.333055	18.830183	-0.050737	1.639627
270.548349	713.484959	18.835187	-0.050704	1.632847
270.676602	705.549121	18.840192	-0.050723	1.626002
270.488981	697.718033	18.845197	-0.050683	1.619175
270.262488	689.907576	18.850202	-0.050635	1.612331
270.257002	682.030441	18.855207	-0.050629	1.605431
270.314933	674.178159	18.860211	-0.050635	1.598532
270.239593	666.341224	18.865216	-0.050616	1.591598
269.977141	658.505204	18.870221	-0.050562	1.584607
270.286797	650.627319	18.875226	-0.050614	1.577631
270.109784	642.804286	18.880231	-0.050576	1.570602
269.918464	634.982157	18.885235	-0.050535	1.563540
270.211663	627.113167	18.890240	-0.050585	1.556475
269.996283	619.286339	18.895245	-0.050540	1.549341
269.902198	611.460509	18.900250	-0.050517	1.542192
269.925721	603.618569	18.905255	-0.050516	1.535013
270.028388	595.769709	18.910259	-0.050530	1.527806
269.920853	587.968970	18.915264	-0.050505	1.520578
269.655164	580.182169	18.920269	-0.050451	1.513304
269.741321	572.327106	18.925274	-0.050462	1.505985
269.685602	564.520417	18.930279	-0.050446	1.498653
269.534276	556.716152	18.935283	-0.050413	1.491273
269.563404	548.897241	18.940288	-0.050413	1.483871
269.514308	541.091922	18.945293	-0.050399	1.476432
269.436803	533.244647	18.950298	-0.050379	1.468910
269.235594	525.455923	18.955303	-0.050337	1.461387
269.434225	517.614505	18.960307	-0.050369	1.453837
269.413006	509.816167	18.965312	-0.050360	1.446255
269.281220	502.050725	18.970317	-0.050330	1.438647
269.309453	494.240419	18.975322	-0.050330	1.430981
269.384891	486.431389	18.980327	-0.050339	1.423282
268.935639	478.724177	18.985331	-0.050250	1.415556
268.995321	470.918187	18.990336	-0.050256	1.407773
268.947845	463.136792	18.995341	-0.050243	1.399954
268.859288	455.370774	19.000346	-0.050221	1.392100
268.781497	447.582700	19.005351	-0.050201	1.384180
268.702186	439.817320	19.010355	-0.050182	1.376238
268.703005	432.039755	19.015360	-0.050177	1.368250
268.491566	424.299598	19.020365	-0.050132	1.360218
268.424046	416.548650	19.025370	-0.050115	1.352152
268.480990	408.761631	19.030375	-0.050120	1.344021
268.204336	401.053465	19.035379	-0.050064	1.335865
268.205169	393.294324	19.040384	-0.050059	1.327655
268.368890	385.516786	19.045389	-0.050084	1.319402
268.274098	377.720884	19.050394	-0.050061	1.311032
268.199538	369.937729	19.055399	-0.050042	1.302625
268.131709	362.222697	19.060403	-0.050025	1.294238
268.126731	354.499740	19.065408	-0.050019	1.285800
268.128382	346.791678	19.070413	-0.050014	1.277324
268.007476	339.091475	19.075418	-0.049986	1.268777
268.077415	331.371289	19.080423	-0.049994	1.260186
267.899133	323.693929	19.085427	-0.049956	1.251536
267.744273	316.016274	19.090432	-0.049922	1.242831
267.664453	308.336346	19.095437	-0.049903	1.234076
267.631878	300.631514	19.100442	-0.049891	1.225239
267.515090	292.967247	19.105447	-0.049865	1.216368
267.491717	285.275317	19.110451	-0.049855	1.207418
267.471145	277.621445	19.115456	-0.049847	1.198447
267.453641	269.944341	19.120461	-0.049838	1.189381
267.143238	262.334937	19.125466	-0.049775	1.180266
267.153943	254.674842	19.130471	-0.049772	1.171086
267.163918	247.021209	19.135475	-0.049769	1.161840
267.034966	239.404005	19.140480	-0.049740	1.152536
267.122868	231.716489	19.145485	-0.049752	1.143115
266.920603	224.132075	19.150490	-0.049709	1.133683
266.791439	216.523184	19.155495	-0.049680	1.124156
266.738005	208.924378	19.160499	-0.049665	1.114577
266.830312	201.303345	19.165504	-0.049677	1.104918
266.645764	193.739631	19.170509	-0.049638	1.095186
266.656854	186.156442	19.175514	-0.049635	1.085386
266.573029	178.610375	19.180519	-0.049615	1.075524
266.415762	171.051455	19.185523	-0.049580	1.065536
266.248836	163.527754	19.190528	-0.049544	1.055499
266.110631	155.986864	19.195533	-0.049514	1.045349
266.035181	148.480740	19.200538	-0.049495	1.035161
266.004718	140.950699	19.205543	-0.049484	1.024850
265.849264	133.465405	19.210547	-0.049450	1.014466
266.000240	125.945693	19.215552	-0.049474	1.004001
265.671059	118.506881	19.220557	-0.049408	0.993422
265.591137	111.013398	19.225562	-0.049388	0.982712
265.542354	103.560423	19.230567	-0.049374	0.971952
265.511519	96.114108	19.235571	-0.049363	0.961085
265.674652	88.661873	19.240576	-0.049389	0.950136
265.473731	81.269876	19.245581	-0.049346	0.939053
265.353637	73.898944	19.250586	-0.049319	0.927892
265.132638	66.562105	19.255591	-0.049273	0.916620
264.983602	59.436142	19.260595	-0.049241	0.905555