Fri Mar 12 12:09:54 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.602284	0.141586	0.000000	0.000024	0.721100
0.704445	0.082812	0.005005	0.000005	0.721021
0.739358	0.007259	0.010010	-0.000002	0.720884
0.681978	0.011334	0.015014	0.000009	0.720872
0.672058	0.017626	0.020019	0.000011	0.720881
0.806093	-0.007745	0.025024	-0.000014	0.720878
0.781383	-0.005879	0.030029	-0.000010	0.720873
0.759039	0.002150	0.035034	-0.000005	0.720881
0.742226	-0.000127	0.040038	-0.000002	0.720871
0.676859	0.014017	0.045043	0.000010	0.720875
0.647460	0.018423	0.050048	0.000015	0.720874
0.588848	0.027318	0.055053	0.000026	0.720871
1.010332	-0.043252	0.060058	-0.000052	0.720880
0.783035	-0.008126	0.065062	-0.000010	0.720869
0.603763	0.028047	0.070067	0.000024	0.720877
0.667432	-0.003436	0.075072	0.000012	0.720838
0.575505	-0.140559	0.080077	0.000029	0.720536
0.613678	-0.146282	0.085082	0.000022	0.720538
0.616969	-0.148846	0.090086	0.000021	0.720534
0.497190	-0.124775	0.095091	0.000044	0.720539
0.534555	-0.131782	0.100096	0.000037	0.720539
0.759094	-0.173429	0.105101	-0.000005	0.720535
0.625754	-0.201848	0.110106	0.000020	0.720433
0.558971	-0.298824	0.115110	0.000032	0.720218
0.624092	-0.306216	0.120115	0.000020	0.720226
0.734732	-0.326707	0.125120	-0.000001	0.720225
0.744441	-0.330810	0.130125	-0.000002	0.720220
0.655453	-0.370947	0.135130	0.000014	0.720110
0.780822	-0.501698	0.140134	-0.000009	0.719896
0.840457	-0.509106	0.145139	-0.000020	0.719903
0.709663	-0.487512	0.150144	0.000004	0.719899
0.660670	-0.515380	0.155149	0.000013	0.719827
0.751226	-0.644442	0.160154	-0.000003	0.719605
0.317268	-0.572379	0.165158	0.000077	0.719594
0.343365	-0.574726	0.170163	0.000073	0.719599
0.456193	-0.652419	0.175168	0.000052	0.719485
0.453111	-0.762376	0.180173	0.000052	0.719267
0.420345	-0.752103	0.185178	0.000058	0.719276
0.371799	-0.746975	0.190182	0.000067	0.719269
0.747492	-0.942755	0.195187	-0.000002	0.719015
0.715966	-0.962019	0.200192	0.000003	0.718966
0.413330	-0.909341	0.205197	0.000060	0.718963
0.556681	-1.052298	0.210202	0.000033	0.718732
0.467995	-1.079481	0.215206	0.000050	0.718647
0.467908	-1.075626	0.220211	0.000050	0.718654
0.573245	-1.220221	0.225216	0.000030	0.718406
0.432342	-1.222275	0.230221	0.000056	0.718352
0.560148	-1.257524	0.235226	0.000033	0.718328
0.655297	-1.433829	0.240230	0.000015	0.718013
0.653770	-1.428694	0.245235	0.000015	0.718022
0.570127	-1.503500	0.250240	0.000031	0.717845
0.601777	-1.583182	0.255245	0.000025	0.717699
0.674596	-1.613128	0.260250	0.000012	0.717665
0.364356	-1.701805	0.265254	0.000069	0.717381
0.327340	-1.693628	0.270259	0.000076	0.717384
0.304799	-1.800387	0.275264	0.000081	0.717165
0.459533	-1.871189	0.280269	0.000052	0.717079
0.173291	-1.888961	0.285274	0.000105	0.716943
0.157070	-1.981831	0.290278	0.000108	0.716754
0.188748	-2.014483	0.295283	0.000102	0.716700
0.337060	-2.167378	0.300288	0.000075	0.716450
0.138492	-2.138664	0.305293	0.000112	0.716437
0.341441	-2.323627	0.310298	0.000074	0.716142
0.154586	-2.295420	0.315302	0.000109	0.716132
-0.057224	-2.375596	0.320307	0.000148	0.715898
-0.052702	-2.380533	0.325312	0.000148	0.715890
-1.537764	-2.267040	0.330317	0.000424	0.715591
-3.306453	-1.970815	0.335322	0.000753	0.715553
-3.520116	-1.936055	0.340326	0.000793	0.715547
-3.196250	-2.105765	0.345331	0.000733	0.715325
-4.503779	-1.917336	0.350336	0.000976	0.715236
-4.166556	-1.980830	0.355341	0.000913	0.715229
-3.727159	-2.072600	0.360346	0.000832	0.715203
-4.976869	-2.002751	0.365350	0.001064	0.714900
-4.688689	-2.048698	0.370355	0.001011	0.714910
-4.992890	-1.994343	0.375360	0.001067	0.714911
-5.329690	-1.937680	0.380365	0.001130	0.714904
-5.086002	-2.121862	0.385370	0.001085	0.714625
-6.008729	-1.968241	0.390374	0.001256	0.714603
-6.140986	-1.943023	0.395379	0.001281	0.714606
-5.587704	-2.040921	0.400384	0.001178	0.714608
-6.156242	-2.023944	0.405389	0.001284	0.714440
-7.008544	-1.951242	0.410394	0.001443	0.714283
-6.548637	-2.037339	0.415398	0.001357	0.714275
-6.898270	-1.974219	0.420403	0.001422	0.714276
-7.045305	-1.947705	0.425408	0.001449	0.714277
-7.183983	-1.976036	0.430413	0.001475	0.714172
-7.711680	-1.982970	0.435418	0.001574	0.713971
-7.551727	-2.014213	0.440422	0.001544	0.713966
-8.077096	-1.916405	0.445427	0.001642	0.713974
-7.813777	-1.964374	0.450432	0.001593	0.713972
-7.727736	-1.983234	0.455437	0.001577	0.713965
-7.867184	-2.065866	0.460442	0.001603	0.713751
-9.145832	-1.890737	0.465446	0.001841	0.713647
-8.421043	-2.016451	0.470451	0.001706	0.713653
-8.408660	-2.018378	0.475456	0.001703	0.713654
-9.043538	-1.908046	0.480461	0.001821	0.713648
-8.505154	-1.999999	0.485466	0.001721	0.713656
-8.627333	-2.097943	0.490470	0.001744	0.713418
-9.907159	-1.899618	0.495475	0.001982	0.713359
-9.609189	-1.952546	0.500480	0.001927	0.713359
-9.503499	-1.975336	0.505485	0.001907	0.713352
-9.424644	-1.983652	0.510490	0.001893	0.713363
-9.602387	-1.955942	0.515494	0.001926	0.713355
-9.492432	-2.073498	0.520499	0.001905	0.713160
-10.564438	-1.950664	0.525504	0.002105	0.713024
-10.553168	-1.954551	0.530509	0.002103	0.713021
-10.149664	-2.022597	0.535514	0.002028	0.713028
-10.585836	-1.949427	0.540518	0.002109	0.713019
-10.570055	-1.949842	0.545523	0.002106	0.713024
-10.355355	-2.010604	0.550528	0.002066	0.712979
-11.173429	-2.003292	0.555533	0.002218	0.712704
-11.122847	-2.005557	0.560538	0.002209	0.712717
-11.751850	-1.898104	0.565542	0.002326	0.712708
-11.224628	-1.989491	0.570547	0.002228	0.712713
-11.044636	-2.021714	0.575552	0.002194	0.712713
-11.790635	-1.891807	0.580557	0.002333	0.712707
-11.403890	-2.017395	0.585562	0.002261	0.712594
-12.218165	-1.978156	0.590566	0.002413	0.712383
-12.064071	-2.005334	0.595571	0.002384	0.712384
-12.551940	-1.915148	0.600576	0.002475	0.712390
-12.774079	-1.879833	0.605581	0.002516	0.712382
-12.005196	-2.012794	0.610586	0.002373	0.712390
-12.289461	-1.966488	0.615590	0.002426	0.712381
-12.110003	-2.050140	0.620595	0.002393	0.712278
-12.662879	-2.045324	0.625600	0.002496	0.712091
-13.169049	-1.959083	0.630605	0.002590	0.712083
-13.060084	-1.974421	0.635610	0.002570	0.712091
-12.802332	-2.022617	0.640614	0.002522	0.712087
-13.001766	-1.986097	0.645619	0.002559	0.712089
-13.166074	-1.955170	0.650624	0.002589	0.712092
-13.594284	-2.021521	0.655629	0.002669	0.711808
-13.773905	-2.009437	0.660634	0.002703	0.711768
-14.281719	-1.923252	0.665638	0.002797	0.711760
-13.912528	-1.987507	0.670643	0.002728	0.711763
-13.858121	-1.996610	0.675648	0.002718	0.711764
-14.041022	-1.967734	0.680653	0.002752	0.711756
-13.949942	-1.979887	0.685658	0.002735	0.711764
-14.484183	-2.021209	0.690662	0.002835	0.711492
-15.078565	-1.935559	0.695667	0.002945	0.711452
-15.353841	-1.884389	0.700672	0.002997	0.711456
-15.196178	-1.914397	0.705677	0.002967	0.711452
-14.881735	-1.967568	0.710682	0.002909	0.711458
-15.106449	-1.930260	0.715686	0.002951	0.711452
-15.219090	-1.907132	0.720691	0.002972	0.711459
-14.750709	-2.025689	0.725696	0.002884	0.711388
-16.051295	-1.921571	0.730701	0.003127	0.711134
-15.833341	-1.954930	0.735706	0.003086	0.711145
-16.111413	-1.909676	0.740710	0.003138	0.711136
-15.677314	-1.984838	0.745715	0.003057	0.711141
-15.785058	-1.965868	0.750720	0.003077	0.711140
-16.078184	-1.918753	0.755725	0.003132	0.711130
-15.543780	-2.025203	0.760730	0.003032	0.711107
-16.627991	-1.951885	0.765734	0.003234	0.710868
-16.678702	-1.941827	0.770739	0.003243	0.710870
-16.464222	-1.979144	0.775744	0.003204	0.710872
-16.426296	-1.987384	0.780749	0.003196	0.710869
-16.612545	-1.951805	0.785754	0.003231	0.710874
-16.660186	-1.945892	0.790758	0.003240	0.710869
-16.245055	-2.098636	0.795763	0.003163	0.710711
-17.579417	-1.949756	0.800768	0.003411	0.710534
-17.692358	-1.932400	0.805773	0.003432	0.710528
-17.276102	-2.004308	0.810778	0.003355	0.710533
-17.614129	-1.946801	0.815782	0.003418	0.710527
-17.762928	-1.920358	0.820787	0.003445	0.710527
-17.631891	-1.941282	0.825792	0.003421	0.710532
-17.669478	-2.008780	0.830797	0.003428	0.710384
-18.632466	-1.919627	0.835802	0.003607	0.710219
-18.235818	-1.991793	0.840806	0.003533	0.710216
-18.335432	-1.973919	0.845811	0.003552	0.710216
-18.439878	-1.953154	0.850816	0.003571	0.710221
-18.470375	-1.952011	0.855821	0.003577	0.710212
-18.185178	-1.998183	0.860826	0.003524	0.710221
-18.470075	-2.034265	0.865830	0.003577	0.710048
-19.716415	-1.890628	0.870835	0.003809	0.709891
-18.970443	-2.021379	0.875840	0.003670	0.709895
-19.271885	-1.971870	0.880845	0.003726	0.709887
-19.342443	-1.954099	0.885850	0.003740	0.709897
-19.299320	-1.966933	0.890854	0.003732	0.709887
-19.313590	-1.963215	0.895859	0.003734	0.709889
-19.517089	-2.000917	0.900864	0.003772	0.709741
-20.702273	-1.865719	0.905869	0.003993	0.709589
-20.007099	-1.985197	0.910874	0.003863	0.709598
-20.126803	-1.964952	0.915878	0.003886	0.709596
-20.500837	-1.898171	0.920883	0.003955	0.709596
-20.132560	-1.961420	0.925888	0.003887	0.709601
-20.249863	-1.945232	0.930893	0.003909	0.709591
-20.171357	-1.998747	0.935898	0.003894	0.709512
-21.178704	-1.942880	0.940902	0.004082	0.709265
-20.824015	-2.007727	0.945907	0.004016	0.709262
-21.034884	-1.967645	0.950912	0.004055	0.709267
-21.341385	-1.917462	0.955917	0.004112	0.709258
-20.835792	-2.003392	0.960922	0.004018	0.709266
-20.876154	-1.998183	0.965926	0.004025	0.709262
-21.184716	-2.005900	0.970931	0.004083	0.709137
-22.105722	-1.929755	0.975936	0.004254	0.708960
-21.889816	-1.972947	0.980941	0.004214	0.708951
-22.011765	-1.945751	0.985946	0.004237	0.708962
-22.085681	-1.936588	0.990950	0.004250	0.708954
-21.712032	-2.003022	0.995955	0.004181	0.708954
-21.772280	-1.988186	1.000960	0.004192	0.708962
-22.353741	-1.924470	1.005965	0.004300	0.708882
-22.845126	-1.956971	1.010970	0.004392	0.708642
-22.497760	-2.021800	1.015974	0.004327	0.708636
-23.139086	-1.906323	1.020979	0.004447	0.708638
-22.870382	-1.950819	1.025984	0.004397	0.708645
-22.528868	-2.016749	1.030989	0.004333	0.708635
-22.928022	-1.941473	1.035994	0.004407	0.708643
-23.154439	-1.925936	1.040998	0.004449	0.708594
-23.317424	-2.019252	1.046003	0.004480	0.708349
-23.302370	-2.018854	1.051008	0.004477	0.708355
-24.158600	-1.870799	1.056013	0.004636	0.708346
-23.745439	-1.940460	1.061018	0.004560	0.708354
-23.473416	-1.991354	1.066022	0.004509	0.708349
-24.017905	-1.895667	1.071027	0.004610	0.708346
-23.676797	-1.988476	1.076032	0.004547	0.708282
-24.689631	-1.946146	1.081037	0.004735	0.708005
-24.422384	-1.990116	1.086042	0.004686	0.708012
-24.797822	-1.925102	1.091046	0.004756	0.708008
-24.590676	-1.961863	1.096051	0.004717	0.708009
-24.444192	-1.985515	1.101056	0.004690	0.708014
-25.022543	-1.886904	1.106061	0.004797	0.708005
-24.598943	-1.959169	1.111066	0.004719	0.708011
-25.072585	-2.031176	1.116070	0.004807	0.707697
-25.765886	-1.908609	1.121075	0.004936	0.707695
-25.668331	-1.923814	1.126080	0.004918	0.707700
-25.466584	-1.964633	1.131085	0.004880	0.707690
-25.269210	-1.994050	1.136090	0.004843	0.707701
-25.697728	-1.920001	1.141094	0.004923	0.707697
-25.434959	-1.967455	1.146099	0.004874	0.707696
-25.719799	-2.065572	1.151104	0.004927	0.707397
-26.628899	-1.918734	1.156109	0.005097	0.707366
-26.712994	-1.900006	1.161114	0.005112	0.707374
-26.324323	-1.971303	1.166118	0.005040	0.707370
-26.559389	-1.929360	1.171123	0.005084	0.707370
-26.689286	-1.902235	1.176128	0.005108	0.707378
-26.435089	-1.950613	1.181133	0.005060	0.707372
-26.456441	-2.043638	1.186138	0.005065	0.707177
-27.612660	-1.889447	1.191142	0.005280	0.707073
-27.259068	-1.951653	1.196147	0.005214	0.707075
-26.984118	-1.996771	1.201152	0.005163	0.707083
-27.422123	-1.923824	1.206157	0.005244	0.707072
-27.187296	-1.960351	1.211162	0.005201	0.707083
-26.903158	-2.013210	1.216166	0.005148	0.707078
-27.790078	-2.002235	1.221171	0.005313	0.706783
-28.194636	-1.942708	1.226176	0.005388	0.706758
-28.319526	-1.927670	1.231181	0.005411	0.706743
-27.681307	-2.036184	1.236186	0.005293	0.706754
-28.326525	-1.921751	1.241190	0.005413	0.706753
-28.319418	-1.925267	1.246195	0.005411	0.706748
-27.732420	-2.026555	1.251200	0.005302	0.706755
-28.648387	-2.019223	1.256205	0.005473	0.706442
-29.038581	-1.948615	1.261210	0.005545	0.706444
-28.728875	-2.005100	1.266214	0.005488	0.706441
-28.890720	-1.978149	1.271219	0.005518	0.706437
-28.911745	-1.969813	1.276224	0.005522	0.706446
-28.944422	-1.969228	1.281229	0.005528	0.706436
-28.821866	-2.038182	1.286234	0.005505	0.706341
-29.927918	-1.949543	1.291238	0.005711	0.706123
-30.040926	-1.930947	1.296243	0.005732	0.706120
-29.805987	-1.967620	1.301248	0.005688	0.706130
-30.118218	-1.917781	1.306253	0.005746	0.706119
-29.908974	-1.950457	1.311258	0.005707	0.706128
-29.848126	-1.960950	1.316262	0.005696	0.706129
-29.953817	-1.945560	1.321267	0.005716	0.706122
-30.223854	-2.023299	1.326272	0.005766	0.705869
-30.857527	-1.916077	1.331277	0.005884	0.705857
-30.608124	-1.960067	1.336282	0.005838	0.705858
-30.362084	-2.004970	1.341286	0.005792	0.705856
-30.689272	-1.947261	1.346291	0.005853	0.705855
-30.650613	-1.949879	1.351296	0.005846	0.705863
-30.587132	-2.039847	1.356301	0.005834	0.705705
-31.911465	-1.893295	1.361306	0.006080	0.705525
-31.686925	-1.934289	1.366310	0.006039	0.705523
-31.566353	-1.958378	1.371315	0.006016	0.705518
-31.604835	-1.946820	1.376320	0.006023	0.705527
-31.681092	-1.939660	1.381325	0.006037	0.705514
-31.518515	-1.965380	1.386330	0.006007	0.705521
-31.520664	-2.005136	1.391334	0.006008	0.705440
-32.650393	-1.921928	1.396339	0.006218	0.705202
-32.147503	-2.006844	1.401344	0.006124	0.705212
-32.744746	-1.905409	1.406349	0.006235	0.705201
-32.665003	-1.917682	1.411354	0.006221	0.705205
-32.485891	-1.949220	1.416358	0.006187	0.705206
-32.528472	-1.940694	1.421363	0.006195	0.705208
-32.426424	-1.988618	1.426368	0.006176	0.705148
-33.443444	-1.940251	1.431373	0.006366	0.704880
-33.178450	-1.985008	1.436378	0.006316	0.704885
-33.389866	-1.947507	1.441382	0.006356	0.704885
-33.591425	-1.914631	1.446387	0.006393	0.704879
-33.295887	-1.963206	1.451392	0.006338	0.704887
-33.557927	-1.922338	1.456397	0.006387	0.704875
-33.559838	-1.915832	1.461402	0.006387	0.704888
-33.846936	-2.009740	1.466406	0.006441	0.704595
-34.229011	-1.948166	1.471411	0.006512	0.704582
-34.296710	-1.931056	1.476416	0.006525	0.704592
-34.378175	-1.921719	1.481421	0.006540	0.704582
-34.511753	-1.894531	1.486426	0.006565	0.704589
-34.237309	-1.944655	1.491430	0.006514	0.704586
-34.548710	-1.889676	1.496435	0.006571	0.704585
-34.417036	-2.038276	1.501440	0.006547	0.704333
-35.300338	-1.920209	1.506445	0.006711	0.704254
-35.240808	-1.928533	1.511450	0.006700	0.704258
-35.091465	-1.956084	1.516454	0.006673	0.704256
-35.391326	-1.904787	1.521459	0.006728	0.704252
-35.011828	-1.968608	1.526464	0.006658	0.704260
-35.257121	-1.928473	1.531469	0.006703	0.704252
-35.769125	-1.953235	1.536474	0.006799	0.704018
-36.281462	-1.894976	1.541478	0.006894	0.703952
-36.421318	-1.872359	1.546483	0.006920	0.703947
-36.094119	-1.927478	1.551488	0.006859	0.703954
-36.078006	-1.933984	1.556493	0.006856	0.703946
-36.142706	-1.921322	1.561498	0.006868	0.703948
-36.035407	-1.938861	1.566502	0.006848	0.703952
-36.298127	-1.954432	1.571507	0.006897	0.703826
-37.007058	-1.919949	1.576512	0.007029	0.703640
-37.033214	-1.920619	1.581517	0.007034	0.703630
-37.008436	-1.922170	1.586522	0.007030	0.703635
-36.788903	-1.961229	1.591526	0.006989	0.703635
-37.206311	-1.889899	1.596531	0.007066	0.703629
-36.984251	-1.926662	1.601536	0.007025	0.703635
-36.705961	-2.031738	1.606541	0.006973	0.703523
-37.542671	-1.974855	1.611546	0.007129	0.703337
-37.509933	-1.977131	1.616550	0.007123	0.703344
-37.842894	-1.922671	1.621555	0.007185	0.703334
-37.833327	-1.919733	1.626560	0.007183	0.703343
-37.732170	-1.944105	1.631565	0.007164	0.703331
-37.616336	-1.961893	1.636570	0.007143	0.703336
-37.879302	-2.051301	1.641574	0.007192	0.703061
-38.798465	-1.918752	1.646579	0.007363	0.702998
-38.546805	-1.958170	1.651584	0.007316	0.703009
-38.299331	-2.006657	1.656589	0.007270	0.703000
-38.609771	-1.949330	1.661594	0.007328	0.703004
-38.719214	-1.929465	1.666598	0.007348	0.703005
-38.492164	-1.999659	1.671603	0.007306	0.702945
-39.303688	-1.977504	1.676608	0.007457	0.702697
-39.702462	-1.909796	1.681613	0.007531	0.702690
-39.657025	-1.915846	1.686618	0.007523	0.702694
-39.169795	-2.003296	1.691622	0.007432	0.702693
-39.741165	-1.905316	1.696627	0.007538	0.702685
-39.513863	-1.939390	1.701632	0.007496	0.702698
-39.783952	-1.901154	1.706637	0.007546	0.702678
-40.031438	-2.010289	1.711642	0.007593	0.702368
-40.204435	-1.980133	1.716646	0.007625	0.702367
-40.588451	-1.913008	1.721651	0.007696	0.702364
-39.999936	-2.014310	1.726656	0.007587	0.702372
-40.236682	-1.975953	1.731661	0.007631	0.702364
-40.372022	-1.948535	1.736666	0.007656	0.702371
-39.942769	-2.084598	1.741670	0.007576	0.702250
-41.426460	-1.909000	1.746675	0.007852	0.702070
-41.089875	-1.965423	1.751680	0.007790	0.702078
-41.156225	-1.957485	1.756685	0.007802	0.702070
-41.135224	-1.958988	1.761690	0.007798	0.702074
-41.158906	-1.956111	1.766694	0.007803	0.702071
-41.389123	-1.917719	1.771699	0.007845	0.702066
-41.235036	-2.036366	1.776704	0.007817	0.701882
-42.460375	-1.889886	1.781709	0.008045	0.701736
-42.089882	-1.952205	1.786714	0.007976	0.701743
-41.529689	-2.051976	1.791718	0.007872	0.701744
-42.262059	-1.923655	1.796723	0.008008	0.701739
-42.168278	-1.936554	1.801728	0.007991	0.701747
-42.065024	-1.959513	1.806733	0.007971	0.701738
-42.059705	-2.055792	1.811738	0.007970	0.701545
-43.056368	-1.929962	1.816742	0.008156	0.701440
-42.939920	-1.954539	1.821747	0.008134	0.701432
-42.519163	-2.024976	1.826752	0.008056	0.701441
-42.853610	-1.969729	1.831757	0.008118	0.701432
-42.884723	-1.962865	1.836762	0.008124	0.701435
-42.658372	-2.006539	1.841766	0.008082	0.701428
-43.448327	-2.021312	1.846771	0.008229	0.701113
-43.588474	-1.992039	1.851776	0.008255	0.701122
-43.556644	-1.999714	1.856781	0.008249	0.701118
-43.400712	-2.026360	1.861786	0.008220	0.701120
-43.526417	-2.002784	1.866790	0.008244	0.701122
-43.778383	-1.961355	1.871795	0.008290	0.701115
-43.545854	-2.068243	1.876800	0.008247	0.700983
-44.530493	-1.948783	1.881805	0.008430	0.700869
-44.595270	-1.935609	1.886810	0.008443	0.700872
-44.261668	-1.993901	1.891814	0.008380	0.700875
-44.505057	-1.953306	1.896819	0.008426	0.700869
-44.512933	-1.948931	1.901824	0.008427	0.700875
-44.406345	-1.971940	1.906829	0.008407	0.700867
-45.049436	-2.017425	1.911834	0.008527	0.700542
-45.226456	-1.988394	1.916838	0.008560	0.700537
-45.653121	-1.914536	1.921843	0.008640	0.700533
-44.995374	-2.026976	1.926848	0.008517	0.700542
-45.325605	-1.970931	1.931853	0.008579	0.700537
-45.651823	-1.912714	1.936858	0.008639	0.700537
-45.254062	-2.007974	1.941862	0.008565	0.700487
-46.049239	-2.001500	1.946867	0.008713	0.700213
-46.144924	-1.979006	1.951872	0.008731	0.700224
-46.325562	-1.951290	1.956877	0.008765	0.700215
-45.993950	-2.008076	1.961882	0.008703	0.700220
-46.219858	-1.967400	1.966886	0.008745	0.700220
-46.549941	-1.912610	1.971891	0.008807	0.700212
-45.987893	-2.063363	1.976896	0.008702	0.700110
-47.107018	-1.971113	1.981901	0.008910	0.699892
-47.106273	-1.969203	1.986906	0.008910	0.699896
-47.105457	-1.968921	1.991910	0.008910	0.699897
-47.101106	-1.973847	1.996915	0.008909	0.699888
-47.283259	-1.937673	2.001920	0.008943	0.699896
-46.974472	-2.045069	2.011917	0.008886	0.699790
-48.103371	-1.938257	2.021914	0.009096	0.699598
-48.079704	-1.943008	2.031910	0.009091	0.699597
-47.918482	-1.972445	2.041907	0.009061	0.699595
-48.128725	-1.933748	2.051904	0.009101	0.699598
-47.862636	-1.981425	2.061901	0.009051	0.699597
-48.195935	-1.921667	2.071898	0.009113	0.699598
-47.935544	-1.943497	2.081894	0.009065	0.699648
-47.191320	-1.955608	2.091891	0.008926	0.699893
-47.043295	-1.980688	2.101888	0.008899	0.699895
-47.122959	-1.965471	2.111885	0.008913	0.699897
-47.219270	-1.949442	2.121882	0.008931	0.699895
-47.088686	-1.973376	2.131878	0.008907	0.699894
-47.309787	-1.933513	2.141875	0.008948	0.699895
-47.165629	-1.959290	2.151872	0.008921	0.699894
-46.566355	-1.926626	2.161869	0.008810	0.700177
-46.388682	-1.938420	2.171866	0.008777	0.700218
-46.021918	-2.004088	2.181862	0.008708	0.700217
-46.391554	-1.938816	2.191859	0.008777	0.700216
-46.359730	-1.900013	2.201856	0.008771	0.700306
-45.330643	-1.969700	2.211853	0.008580	0.700537
-45.394748	-1.959262	2.221850	0.008592	0.700535
-45.492775	-1.941965	2.231846	0.008610	0.700534
-45.424526	-1.911217	2.241843	0.008597	0.700621
-44.465083	-1.957127	2.251840	0.008419	0.700875
-44.238519	-1.997366	2.261837	0.008376	0.700875
-44.704267	-1.915498	2.271834	0.008463	0.700873
-44.344857	-1.941125	2.281830	0.008396	0.700951
-43.937334	-1.930377	2.291827	0.008320	0.701120
-43.882593	-1.939513	2.301824	0.008310	0.701121
-43.853343	-1.944682	2.311821	0.008305	0.701121
-43.201059	-1.916419	2.321818	0.008183	0.701414
-42.872563	-1.964449	2.331814	0.008122	0.701435
-43.018082	-1.937989	2.341811	0.008149	0.701436
-42.746592	-1.922228	2.351808	0.008099	0.701566
-42.077474	-1.952872	2.361805	0.007974	0.701746
-41.933406	-1.979171	2.371802	0.007947	0.701744
-42.177190	-1.937584	2.381798	0.007993	0.701740
-41.371847	-1.921407	2.391795	0.007843	0.702064
-41.118559	-1.961693	2.401792	0.007796	0.702074
-41.087615	-1.967473	2.411789	0.007790	0.702073
-41.119498	-1.902423	2.421786	0.007796	0.702193
-40.403712	-1.943079	2.431782	0.007663	0.702369
-40.335760	-1.954800	2.441779	0.007650	0.702370
-40.352333	-1.944492	2.451776	0.007653	0.702385
-39.760179	-1.897219	2.461773	0.007543	0.702693
-39.587690	-1.927927	2.471770	0.007511	0.702694
-39.601810	-1.925787	2.481766	0.007513	0.702693
-39.338175	-1.856198	2.491763	0.007464	0.702928
-38.805565	-1.911921	2.501760	0.007365	0.703008
-38.783952	-1.915341	2.511757	0.007361	0.703008
-38.466055	-1.887921	2.521754	0.007302	0.703178
-37.754923	-1.933766	2.531750	0.007169	0.703342
-37.734239	-1.937639	2.541747	0.007166	0.703341
-37.440125	-1.990147	2.551744	0.007111	0.703341
-37.036234	-1.947772	2.561741	0.007036	0.703572
-36.832099	-1.953061	2.571738	0.006998	0.703635
-36.926906	-1.936846	2.581734	0.007015	0.703633
-36.996266	-1.885313	2.591731	0.007028	0.703712
-35.992465	-1.947042	2.601728	0.006841	0.703949
-36.045827	-1.935892	2.611725	0.006851	0.703952
-36.040757	-1.936400	2.621722	0.006850	0.703953
-35.502741	-1.900078	2.631718	0.006750	0.704219
-35.103132	-1.951505	2.641715	0.006676	0.704259
-34.960084	-1.975526	2.651712	0.006649	0.704262
-35.171352	-1.889624	2.661709	0.006688	0.704360
-33.988554	-1.986944	2.671706	0.006468	0.704588
-34.195702	-1.951246	2.681702	0.006507	0.704586
-34.294134	-1.932448	2.691699	0.006525	0.704588
-33.709267	-1.930073	2.701696	0.006416	0.704803
-33.517719	-1.922658	2.711693	0.006381	0.704887
-33.409035	-1.942103	2.721690	0.006360	0.704887
-33.436138	-1.887399	2.731686	0.006365	0.704987
-32.384080	-1.965916	2.741683	0.006170	0.705207
-32.473912	-1.948923	2.751680	0.006186	0.705209
-32.599277	-1.925750	2.761677	0.006210	0.705210
-31.749743	-1.949833	2.771674	0.006051	0.705467
-31.814034	-1.910633	2.781670	0.006063	0.705522
-31.736401	-1.924775	2.791667	0.006049	0.705522
-31.503157	-1.898489	2.801664	0.006006	0.705658
-30.634655	-1.951356	2.811661	0.005844	0.705863
-30.754531	-1.930988	2.821658	0.005866	0.705861
-30.779538	-1.928037	2.831654	0.005871	0.705858
-30.101772	-1.943916	2.841651	0.005745	0.706069
-30.125619	-1.910775	2.851648	0.005749	0.706127
-29.996022	-1.932974	2.861645	0.005725	0.706129
-29.759893	-1.900880	2.871642	0.005681	0.706278
-29.180926	-1.922765	2.881638	0.005573	0.706442
-29.027694	-1.949526	2.891635	0.005545	0.706443
-29.136266	-1.915657	2.901632	0.005565	0.706472
-28.116641	-1.957434	2.911629	0.005375	0.706753
-28.156689	-1.951415	2.921626	0.005383	0.706751
-28.177147	-1.947721	2.931622	0.005386	0.706751
-27.958307	-1.913214	2.941619	0.005346	0.706899
-27.155050	-1.965189	2.951616	0.005196	0.707082
-27.221052	-1.951547	2.961613	0.005208	0.707085
-27.330518	-1.933856	2.971610	0.005229	0.707082
-26.563895	-1.931804	2.981606	0.005086	0.707360
-26.234206	-1.983629	2.991603	0.005025	0.707374
-26.491323	-1.936466	3.001600	0.005073	0.707377
-26.181066	-1.926130	3.011597	0.005015	0.707508
-25.388241	-1.972845	3.021594	0.004867	0.707698
-25.503825	-1.952546	3.031590	0.004889	0.707698
-25.481264	-1.956637	3.041587	0.004885	0.707697
-24.828100	-1.943000	3.051584	0.004763	0.707958
-24.751359	-1.930670	3.061581	0.004749	0.708010
-24.618499	-1.955901	3.071578	0.004724	0.708007
-24.575517	-1.905739	3.081574	0.004716	0.708123
-23.484127	-1.989196	3.091571	0.004513	0.708346
-23.699084	-1.950875	3.101568	0.004553	0.708346
-23.726972	-1.944453	3.111565	0.004558	0.708349
-23.047392	-1.954979	3.121562	0.004431	0.708570
-23.115484	-1.912832	3.131558	0.004444	0.708630
-22.930453	-1.945020	3.141555	0.004410	0.708632
-22.863132	-1.891923	3.151552	0.004397	0.708762
-21.808935	-1.983082	3.161549	0.004201	0.708956
-22.348257	-1.888084	3.171546	0.004301	0.708954
-22.217093	-1.903606	3.181542	0.004277	0.708969
-21.406063	-1.902698	3.191539	0.004126	0.709260
-21.287062	-1.922609	3.201536	0.004104	0.709263
-21.048044	-1.964808	3.211533	0.004059	0.709264
-20.888950	-1.883667	3.221530	0.004030	0.709483
-20.376469	-1.919981	3.231526	0.003934	0.709593
-20.241749	-1.943435	3.241523	0.003909	0.709594
-20.244734	-1.916050	3.251520	0.003910	0.709648
-19.387138	-1.946313	3.261517	0.003750	0.709893
-19.523955	-1.922625	3.271514	0.003775	0.709891
-19.495007	-1.928713	3.281510	0.003770	0.709889
-19.089220	-1.882949	3.291507	0.003695	0.710125
-18.795684	-1.887893	3.301504	0.003640	0.710220
-18.501153	-1.939630	3.311501	0.003585	0.710221
-18.640718	-1.864177	3.321498	0.003611	0.710323
-17.548330	-1.954504	3.331494	0.003408	0.710531
-17.817397	-1.906116	3.341491	0.003458	0.710532
-17.525931	-1.958596	3.351488	0.003404	0.710531
-16.931079	-1.936817	3.361485	0.003293	0.710786
-16.935738	-1.893859	3.371482	0.003294	0.710870
-16.635800	-1.948357	3.381478	0.003238	0.710868
-16.717715	-1.921459	3.391475	0.003253	0.710892
-15.864745	-1.950854	3.401472	0.003094	0.711137
-15.914234	-1.941870	3.411469	0.003103	0.711137
-16.057772	-1.916557	3.421466	0.003130	0.711137
-15.482442	-1.920250	3.431462	0.003023	0.711334
-15.295806	-1.894930	3.441459	0.002988	0.711451
-14.984275	-1.949337	3.451456	0.002930	0.711453
-15.052407	-1.906586	3.461453	0.002943	0.711514
-14.342020	-1.909555	3.471450	0.002811	0.711761
-14.019014	-1.968435	3.481446	0.002751	0.711758
-14.304490	-1.916813	3.491443	0.002804	0.711759
-13.578546	-1.928780	3.501440	0.002669	0.711993
-13.477765	-1.898182	3.511437	0.002650	0.712090
-13.490447	-1.896854	3.521434	0.002652	0.712088
-13.426628	-1.856251	3.531430	0.002640	0.712192
-12.311486	-1.957774	3.541427	0.002433	0.712385
-12.341049	-1.950810	3.551424	0.002438	0.712389
-12.496977	-1.923646	3.561421	0.002467	0.712387
-11.958431	-1.888881	3.571418	0.002367	0.712648
-11.696054	-1.905753	3.581414	0.002318	0.712707
-11.673022	-1.909102	3.591411	0.002314	0.712709
-11.270981	-1.920823	3.601408	0.002239	0.712828
-10.398333	-1.976564	3.611405	0.002077	0.713027
-10.239298	-2.006777	3.621402	0.002047	0.713023
-10.541728	-1.953786	3.631398	0.002103	0.713021
-10.277346	-1.934430	3.641395	0.002054	0.713153
-9.287060	-2.005815	3.651392	0.001870	0.713362
-9.641980	-1.943631	3.661389	0.001936	0.713360
-9.474198	-1.973634	3.671386	0.001905	0.713360
-8.975157	-1.978014	3.681382	0.001812	0.713528
-8.472279	-2.006209	3.691379	0.001718	0.713650
-8.366515	-2.024533	3.701376	0.001698	0.713651
-8.517021	-1.997276	3.711373	0.001726	0.713652
-8.049359	-1.987220	3.721370	0.001639	0.713837
-7.615988	-2.000091	3.731366	0.001559	0.713965
-7.732023	-1.978859	3.741363	0.001580	0.713966
-7.233820	-2.067690	3.751360	0.001488	0.713966
-7.129617	-1.971435	3.761357	0.001468	0.714194
-6.828555	-1.983361	3.771354	0.001412	0.714277
-6.962846	-1.960490	3.781350	0.001437	0.714275
-6.605309	-1.985974	3.791347	0.001371	0.714351
-5.655860	-2.026148	3.801344	0.001194	0.714607
-5.631914	-2.029854	3.811341	0.001189	0.714608
-5.633391	-2.030566	3.821338	0.001190	0.714606
-5.616406	-1.974534	3.831334	0.001186	0.714723
-4.681108	-2.047635	3.841331	0.001012	0.714909
-4.860570	-2.016049	3.851328	0.001046	0.714908
-4.866692	-2.015107	3.861325	0.001047	0.714908
-4.140007	-2.027577	3.871322	0.000912	0.715140
-4.096096	-1.990164	3.881318	0.000903	0.715230
-3.777399	-2.046063	3.891315	0.000844	0.715232
-3.826638	-2.037519	3.901312	0.000853	0.715231
-3.240856	-1.990303	3.911309	0.000744	0.715532
-2.844284	-2.053372	3.921306	0.000670	0.715547
-3.115261	-2.007535	3.931302	0.000721	0.715542
-2.748568	-2.027517	3.941299	0.000653	0.715632
-2.095774	-2.015612	3.951296	0.000531	0.715886
-2.076311	-2.018479	3.961293	0.000527	0.715887
-2.121186	-2.010397	3.971290	0.000536	0.715887
-1.800687	-1.989269	3.981286	0.000476	0.716042
-1.503335	-1.996588	3.991283	0.000421	0.716132
-1.489176	-1.996853	4.001280	0.000418	0.716137
-1.264576	-1.976764	4.011277	0.000376	0.716256
-1.086884	-1.910854	4.021274	0.000343	0.716449
-1.047600	-1.917804	4.031270	0.000336	0.716449
-0.976032	-1.845951	4.041267	0.000323	0.716617
-0.843609	-1.799055	4.051264	0.000298	0.716756
-1.005484	-1.745888	4.061261	0.000328	0.716804
-1.085183	-1.588628	4.071258	0.000343	0.717087
-1.141901	-1.554102	4.081254	0.000353	0.717136
-0.803462	-1.490659	4.091251	0.000290	0.717380
-0.688441	-1.460588	4.101248	0.000269	0.717480
-0.782298	-1.330800	4.111245	0.000286	0.717704
-0.593120	-1.268791	4.121242	0.000251	0.717893
-0.571019	-1.207734	4.131238	0.000247	0.718021
-0.785851	-1.006336	4.141235	0.000287	0.718344
-0.743645	-0.931443	4.151232	0.000279	0.718506
-0.738027	-0.833822	4.161229	0.000278	0.718701
-0.680416	-0.710659	4.171226	0.000267	0.718964
-0.632045	-0.585129	4.181222	0.000258	0.719229
-0.557763	-0.472407	4.191219	0.000244	0.719477
-0.465716	-0.360823	4.201216	0.000227	0.719729
-0.376716	-0.246708	4.211213	0.000210	0.719986
-0.253884	-0.129563	4.221210	0.000187	0.720259
-0.161281	-0.004600	4.231206	0.000170	0.720538
-0.222402	0.178332	4.241203	0.000181	0.720877
0.000000	0.277125	4.251200	0.000140	0.721149
0.089879	0.872875	4.256205	0.000122	0.722351
0.109081	2.138611	4.261210	0.000118	0.724839
0.161192	3.976957	4.266214	0.000107	0.728446
0.491371	6.323467	4.271219	0.000044	0.733115
0.827401	9.182269	4.276224	-0.000020	0.738741
1.030298	12.533905	4.281229	-0.000060	0.745217
1.407572	16.320626	4.286234	-0.000133	0.752517
1.881980	20.490747	4.291238	-0.000224	0.760495
2.213924	25.081798	4.296243	-0.000289	0.769119
2.589227	30.042652	4.301248	-0.000362	0.778336
3.053426	35.323780	4.306253	-0.000452	0.788050
3.288677	40.968884	4.311258	-0.000499	0.798220
3.783306	46.870136	4.316262	-0.000595	0.808792
4.286461	53.047793	4.321267	-0.000693	0.819708
4.788910	59.509623	4.326272	-0.000791	0.830966
5.143480	66.211800	4.331277	-0.000861	0.842433
5.671658	73.109677	4.336282	-0.000964	0.854123
6.256540	80.204163	4.341286	-0.001077	0.865992
7.544598	87.358396	4.346291	-0.001322	0.877998
13.052326	94.013994	4.351296	-0.002352	0.890227
13.634146	101.733279	4.356301	-0.002465	0.902601
13.926369	109.646397	4.361306	-0.002525	0.915028
14.316078	117.637633	4.366310	-0.002602	0.927434
15.384555	125.629241	4.371315	-0.002807	0.939856
16.959652	133.661990	4.376320	-0.003105	0.952308
17.583953	141.929476	4.381325	-0.003227	0.964700
18.519876	150.243003	4.386330	-0.003406	0.977079
19.574066	158.617891	4.391334	-0.003608	0.989421
20.267421	167.091745	4.396339	-0.003743	1.001661
21.320486	175.536401	4.401344	-0.003944	1.013800
22.062272	184.065418	4.406349	-0.004088	1.025836
23.079438	192.596187	4.411354	-0.004283	1.037800
23.680059	201.224019	4.416358	-0.004400	1.049661
24.346301	209.854385	4.421363	-0.004530	1.061407
25.894597	218.384006	4.426368	-0.004824	1.073093
26.670961	227.031860	4.431373	-0.004974	1.084632
27.367818	235.711100	4.436378	-0.005110	1.096072
28.882748	244.247874	4.441382	-0.005397	1.107392
29.067505	253.019425	4.446387	-0.005437	1.118603
29.967795	261.671455	4.451392	-0.005611	1.129708
30.685455	270.341935	4.456397	-0.005750	1.140688
31.280684	279.051470	4.461402	-0.005866	1.151585
32.541920	287.624708	4.466406	-0.006107	1.162353
33.258634	296.268779	4.471411	-0.006246	1.172994
33.692424	304.946099	4.476416	-0.006332	1.183521
34.544556	313.535253	4.481421	-0.006497	1.193935
34.926826	322.180118	4.486426	-0.006573	1.204230
35.703186	330.758185	4.491430	-0.006724	1.214438
36.433896	339.325671	4.496435	-0.006865	1.224539
36.915063	347.957871	4.501440	-0.006960	1.234583
37.503963	356.499698	4.506445	-0.007076	1.244463
38.637314	364.963667	4.511450	-0.007292	1.254282
39.117080	373.517018	4.516454	-0.007387	1.264000
39.918548	382.009711	4.521459	-0.007542	1.273636
40.938332	390.453253	4.526464	-0.007737	1.283186
41.712812	398.934950	4.531469	-0.007887	1.292662
42.363468	407.422624	4.536474	-0.008014	1.302052
43.217445	415.946836	4.541478	-0.008178	1.311451
43.526768	424.488892	4.546483	-0.008241	1.320704
44.226869	432.912159	4.551488	-0.008377	1.329835
44.641446	441.366807	4.556493	-0.008460	1.338887
45.520149	449.727900	4.561498	-0.008629	1.347860
46.600397	458.071765	4.566502	-0.008835	1.356791
47.270706	466.438383	4.571507	-0.008966	1.365616
48.063719	474.816966	4.576512	-0.009119	1.374418
48.447178	483.228730	4.581517	-0.009196	1.383127
49.075988	491.617122	4.586522	-0.009318	1.391799
49.452780	500.010857	4.591526	-0.009394	1.400381
50.056155	508.335380	4.596531	-0.009512	1.408878
50.943647	516.655536	4.601536	-0.009682	1.417367
51.901824	524.927429	4.606541	-0.009866	1.425768
52.551522	533.278798	4.611546	-0.009993	1.434148
52.965286	541.633384	4.616550	-0.010075	1.442444
53.494314	549.951419	4.621555	-0.010179	1.450675
54.335507	558.235963	4.626560	-0.010341	1.458877
54.829343	566.561528	4.631565	-0.010438	1.467017
55.360683	574.922404	4.636570	-0.010543	1.475152
56.102381	583.184623	4.641574	-0.010686	1.483180
56.241875	591.519692	4.646579	-0.010718	1.491141
56.673888	599.823360	4.651584	-0.010803	1.499075
57.175840	608.083016	4.656589	-0.010902	1.506937
57.942945	616.324269	4.661594	-0.011050	1.514780
58.754279	624.542341	4.666598	-0.011207	1.522568
59.081116	632.832759	4.671603	-0.011273	1.530310
59.773467	641.083402	4.676608	-0.011407	1.538031
60.056072	649.351057	4.681613	-0.011465	1.545668
60.183441	657.686529	4.686618	-0.011495	1.553306
61.073227	665.851832	4.691622	-0.011666	1.560864
61.366165	674.103453	4.696627	-0.011726	1.568377
61.653285	682.381747	4.701632	-0.011784	1.575876
62.268701	690.568957	4.706637	-0.011904	1.583306
62.815568	698.787151	4.711642	-0.012011	1.590719
63.377904	707.019162	4.716646	-0.012122	1.598111
63.562823	715.249912	4.721651	-0.012161	1.605415
64.679258	723.389817	4.726656	-0.012375	1.612737
65.297360	731.588038	4.731661	-0.012495	1.620006
65.635797	739.823014	4.736666	-0.012563	1.627236
66.495155	748.048753	4.741670	-0.012729	1.634498
67.414348	756.168262	4.746675	-0.012905	1.641644
68.025719	764.366002	4.751680	-0.013024	1.648784
68.057426	772.647725	4.756685	-0.013036	1.655886
68.601595	780.820009	4.761690	-0.013142	1.662933
69.225880	789.018190	4.766694	-0.013264	1.669984
69.493373	797.241762	4.771699	-0.013319	1.676978
69.977637	805.422228	4.776704	-0.013414	1.683936
70.817783	813.564204	4.781709	-0.013576	1.690880
71.184313	821.774409	4.786714	-0.013650	1.697789
71.754738	829.945350	4.791718	-0.013761	1.704665
72.359453	838.117342	4.796723	-0.013879	1.711518
73.056902	846.276525	4.801728	-0.014014	1.718345
73.417814	854.441168	4.806733	-0.014087	1.725106
73.850281	862.631982	4.811738	-0.014173	1.731871
74.210379	870.840388	4.816742	-0.014245	1.738614
74.645238	878.974686	4.821747	-0.014331	1.745281
74.818425	887.206979	4.826752	-0.014369	1.751968
75.282714	895.362843	4.831757	-0.014461	1.758605
75.457728	903.531885	4.836762	-0.014499	1.765191
75.878307	911.698273	4.841766	-0.014582	1.771781
76.325367	919.840414	4.846771	-0.014671	1.778331
76.838887	927.981854	4.851776	-0.014772	1.784864
77.198358	936.178552	4.856781	-0.014844	1.791398
77.743665	944.323229	4.861786	-0.014951	1.797889
78.569925	952.394523	4.866790	-0.015110	1.804334
79.112240	960.512636	4.871795	-0.015216	1.810757
79.392337	968.709428	4.876800	-0.015274	1.817188
79.658754	976.856624	4.881805	-0.015329	1.823556
80.034035	984.999065	4.886810	-0.015404	1.829910
80.525145	993.149341	4.891814	-0.015501	1.836263
80.805278	1001.284947	4.896819	-0.015558	1.842557
81.212922	1009.434604	4.901824	-0.015639	1.848855
81.492035	1017.596145	4.906829	-0.015697	1.855126
81.891481	1025.713394	4.911834	-0.015776	1.861356
82.525793	1033.832844	4.916838	-0.015900	1.867594
83.032633	1041.970571	4.921843	-0.015999	1.873810
83.398208	1050.103642	4.926848	-0.016073	1.879985
83.880651	1058.215028	4.931853	-0.016168	1.886138
84.421993	1066.326875	4.936858	-0.016274	1.892277
85.061659	1074.449391	4.941862	-0.016398	1.898415
85.361768	1082.568363	4.946867	-0.016459	1.904493
85.824887	1090.702992	4.951872	-0.016551	1.910581
86.189929	1098.842264	4.956877	-0.016624	1.916642
86.717180	1106.930769	4.961882	-0.016728	1.922664
87.067418	1115.085647	4.966886	-0.016798	1.928697
87.411001	1123.220017	4.971891	-0.016868	1.934694
87.645759	1131.367000	4.976896	-0.016917	1.940671
88.225337	1139.456383	4.981901	-0.017030	1.946625
88.471826	1147.632878	4.986906	-0.017081	1.952587
89.018762	1155.735141	4.991910	-0.017188	1.958510
89.316853	1163.816893	4.996915	-0.017249	1.964374
90.040071	1171.881693	5.001920	-0.017389	1.970253
90.367458	1180.023322	5.006925	-0.017455	1.976127
90.647049	1188.132544	5.011930	-0.017512	1.981956
91.111517	1196.242977	5.016934	-0.017604	1.987788
91.284277	1204.391538	5.021939	-0.017642	1.993599
91.681467	1212.477787	5.026944	-0.017721	1.999372
92.009599	1220.576764	5.031949	-0.017787	2.005131
92.243248	1228.696003	5.036954	-0.017836	2.010877
92.695262	1236.805499	5.041958	-0.017925	2.016623
92.971312	1244.902705	5.046963	-0.017982	2.022325
93.405229	1253.004873	5.051968	-0.018068	2.028031
93.900504	1261.130617	5.056973	-0.018166	2.033744
94.415316	1269.187666	5.061978	-0.018267	2.039395
95.383432	1277.214443	5.066982	-0.018452	2.045055
95.915206	1285.320120	5.071987	-0.018557	2.050710
96.222558	1293.459942	5.076992	-0.018619	2.056349
96.746686	1301.544254	5.081997	-0.018722	2.061957
96.889240	1309.681213	5.087002	-0.018754	2.067548
97.435858	1317.793951	5.092006	-0.018861	2.073147
97.997090	1325.850115	5.097011	-0.018971	2.078693
98.302284	1333.953094	5.102016	-0.019033	2.084232
98.740166	1342.052608	5.107021	-0.019119	2.089766
99.101102	1350.162001	5.112026	-0.019192	2.095285
99.669950	1358.238837	5.117030	-0.019303	2.100787
99.922782	1366.336100	5.122035	-0.019356	2.106258
100.177292	1374.511236	5.127040	-0.019408	2.111767
100.599307	1382.625125	5.132045	-0.019492	2.117236
101.020981	1390.660147	5.137050	-0.019576	2.122639
101.338701	1398.751369	5.142054	-0.019640	2.128056
101.690157	1406.840725	5.147059	-0.019711	2.133461
102.233909	1414.907698	5.152064	-0.019817	2.138855
102.565173	1422.987833	5.157069	-0.019884	2.144224
102.654981	1431.108821	5.162074	-0.019906	2.149584
103.209140	1439.189011	5.167078	-0.020015	2.154947
103.657218	1447.236495	5.172083	-0.020104	2.160266
103.934205	1455.339065	5.177088	-0.020160	2.165591
104.463048	1463.410376	5.182093	-0.020264	2.170906
104.933796	1471.483722	5.187098	-0.020357	2.176204
105.270844	1479.585977	5.192102	-0.020425	2.181496
105.416787	1487.696171	5.197107	-0.020458	2.186762
105.974512	1495.784671	5.202112	-0.020567	2.192039
106.332710	1503.881047	5.207117	-0.020639	2.197290
106.549892	1511.942847	5.212122	-0.020684	2.202494
107.137280	1519.997758	5.217126	-0.020799	2.207714
107.497900	1528.081148	5.222131	-0.020871	2.212920
107.658955	1536.198198	5.227136	-0.020907	2.218117
107.990156	1544.268326	5.232141	-0.020974	2.223287
108.462994	1552.316976	5.237146	-0.021067	2.228444
108.972478	1560.421399	5.242150	-0.021167	2.233627
109.267696	1568.489497	5.247155	-0.021227	2.238757
109.881308	1576.518253	5.252160	-0.021347	2.243878
110.233575	1584.615638	5.257165	-0.021418	2.249007
110.505355	1592.725815	5.262170	-0.021473	2.254125
110.867246	1600.803707	5.267174	-0.021546	2.259220
111.096215	1608.879070	5.272179	-0.021594	2.264290
111.692353	1616.926565	5.277184	-0.021710	2.269362
112.280767	1625.079673	5.282189	-0.021825	2.274489
112.881429	1633.075304	5.287194	-0.021942	2.279507
113.302419	1641.152619	5.292198	-0.022026	2.284549
113.510066	1649.232510	5.297203	-0.022070	2.289563
113.960101	1657.306785	5.302208	-0.022159	2.294583
114.309813	1665.368693	5.307213	-0.022229	2.299577
114.690969	1673.430836	5.312218	-0.022305	2.304562
115.307218	1681.482824	5.317222	-0.022425	2.309549
115.539257	1689.596297	5.322227	-0.022474	2.314532
115.847654	1697.658103	5.327232	-0.022536	2.319478
116.283147	1705.716149	5.332237	-0.022623	2.324422
116.712314	1713.769896	5.337242	-0.022708	2.329352
117.153136	1721.862101	5.342246	-0.022795	2.334296
117.301943	1729.953096	5.347251	-0.022828	2.339205
117.528186	1738.023265	5.352256	-0.022876	2.344097
117.966433	1746.099107	5.357261	-0.022963	2.349000
118.150007	1754.204238	5.362266	-0.023002	2.353889
118.475258	1762.269462	5.367270	-0.023068	2.358756
118.801748	1770.306266	5.372275	-0.023134	2.363595
119.099686	1778.371985	5.377280	-0.023195	2.368440
119.212051	1786.489083	5.382285	-0.023221	2.373290
119.600252	1794.510481	5.387290	-0.023298	2.378096
119.961421	1802.556996	5.392294	-0.023371	2.382904
120.232270	1810.633956	5.397299	-0.023426	2.387714
120.543521	1818.735724	5.402304	-0.023490	2.392531
120.762439	1826.810263	5.407309	-0.023536	2.397316
121.107000	1834.845088	5.412314	-0.023605	2.402078
121.365080	1842.924879	5.417318	-0.023658	2.406849
121.903306	1850.953823	5.422323	-0.023764	2.411603
122.207640	1859.036957	5.427328	-0.023826	2.416362
122.803909	1867.058248	5.432333	-0.023942	2.421097
123.250225	1875.085493	5.437338	-0.024030	2.425815
123.649768	1883.189857	5.442342	-0.024110	2.430565
124.067095	1891.306924	5.447347	-0.024193	2.435314
124.373936	1899.336142	5.452352	-0.024255	2.439994
124.681698	1907.368180	5.457357	-0.024318	2.444667
124.980751	1915.418290	5.462362	-0.024379	2.449341
125.582101	1923.488762	5.467366	-0.024496	2.454041
126.172082	1931.506554	5.472371	-0.024611	2.458700
126.210249	1939.598781	5.477376	-0.024624	2.463352
126.444991	1947.688299	5.482381	-0.024672	2.468008
126.677781	1955.751738	5.487386	-0.024721	2.472640
127.065923	1963.820076	5.492390	-0.024799	2.477278
127.254998	1971.861981	5.497395	-0.024839	2.481877
127.601074	1979.909262	5.502400	-0.024909	2.486482
128.227816	1987.959245	5.507405	-0.025031	2.491101
128.506545	1996.022765	5.512410	-0.025088	2.495693
129.053073	2004.052639	5.517414	-0.025195	2.500278
129.566533	2012.080296	5.522419	-0.025296	2.504850
129.628836	2020.204072	5.527424	-0.025313	2.509435
130.104122	2028.292411	5.532429	-0.025406	2.514022
130.498562	2036.309429	5.537434	-0.025485	2.518554
130.943662	2044.346906	5.542438	-0.025573	2.523093
131.095905	2052.417940	5.547443	-0.025607	2.527622
131.054078	2060.524449	5.552448	-0.025604	2.532149
131.331083	2068.582621	5.557453	-0.025661	2.536663
131.554303	2076.633279	5.562458	-0.025708	2.541161
132.023043	2084.656985	5.567462	-0.025800	2.545654
132.466881	2092.703397	5.572467	-0.025888	2.550149
132.765123	2100.775709	5.577472	-0.025949	2.554640
133.032715	2108.836062	5.582477	-0.026004	2.559115
133.124080	2116.878911	5.587482	-0.026026	2.563560
133.626363	2124.930122	5.592486	-0.026125	2.568031
133.948128	2132.988324	5.597491	-0.026190	2.572484
134.390301	2141.027611	5.602496	-0.026278	2.576928
134.895571	2149.067421	5.607501	-0.026377	2.581369
135.097394	2157.116067	5.612506	-0.026420	2.585786
135.633010	2165.172255	5.617510	-0.026525	2.590223
135.813306	2173.432043	5.622515	-0.026564	2.594739
136.326965	2181.395439	5.627520	-0.026665	2.599108
136.943472	2189.368064	5.632525	-0.026785	2.603481
137.204389	2197.397022	5.637530	-0.026838	2.607854
137.492664	2205.472571	5.642534	-0.026897	2.612246
137.605028	2213.541247	5.647539	-0.026924	2.616616
137.697674	2221.585112	5.652544	-0.026946	2.620963
138.057923	2229.621174	5.657549	-0.027018	2.625317
138.326331	2237.639159	5.662554	-0.027074	2.629648
138.495050	2245.729956	5.667558	-0.027110	2.634003
138.830945	2253.762964	5.672563	-0.027178	2.638332
139.257395	2261.769634	5.677568	-0.027263	2.642646
139.549298	2269.823120	5.682573	-0.027322	2.646968
139.641398	2277.887791	5.687578	-0.027345	2.651277
140.378788	2285.923056	5.692582	-0.027487	2.655604
140.723207	2293.964646	5.697587	-0.027557	2.659903
141.142105	2301.992126	5.702592	-0.027640	2.664192
141.691961	2310.036893	5.707597	-0.027747	2.668491
141.801372	2318.140837	5.712602	-0.027773	2.672786
142.146602	2326.212707	5.717606	-0.027843	2.677073
142.539798	2334.214312	5.722611	-0.027921	2.681318
142.915222	2342.237512	5.727616	-0.027996	2.685567
143.143930	2350.303254	5.732621	-0.028044	2.689823
143.383354	2358.365143	5.737626	-0.028094	2.694070
143.616520	2366.444828	5.742630	-0.028142	2.698319
143.738939	2374.473682	5.747635	-0.028171	2.702528
143.743907	2382.548963	5.752640	-0.028177	2.706748
144.474218	2390.563123	5.757645	-0.028318	2.710974
144.701260	2398.637224	5.762650	-0.028365	2.715193
145.090377	2406.655401	5.767654	-0.028443	2.719387
145.501566	2414.684759	5.772659	-0.028525	2.723581
146.042288	2422.704088	5.777664	-0.028631	2.727772
146.363356	2430.789335	5.782669	-0.028696	2.731977
146.292401	2438.875704	5.787674	-0.028688	2.736152
146.693077	2446.918528	5.792678	-0.028768	2.740326
146.719605	2454.952605	5.797683	-0.028778	2.744467
146.827944	2463.022585	5.802688	-0.028803	2.748625
147.146846	2471.149985	5.807693	-0.028868	2.752820
147.380010	2479.166651	5.812698	-0.028917	2.756945
147.479904	2487.186718	5.817702	-0.028940	2.761059
147.815944	2495.174617	5.822707	-0.029008	2.765163
148.098790	2503.184482	5.827712	-0.029066	2.769270
148.456687	2511.267494	5.832717	-0.029138	2.773412
148.344103	2519.316435	5.837722	-0.029122	2.777503
148.688595	2527.352213	5.842726	-0.029192	2.781608
148.890230	2535.379745	5.847731	-0.029234	2.785695
149.381837	2543.386134	5.852736	-0.029331	2.789781
149.775008	2551.458555	5.857741	-0.029410	2.793890
150.150428	2559.478985	5.862746	-0.029485	2.797964
150.248033	2567.539083	5.867750	-0.029508	2.802037
150.344966	2575.585625	5.872755	-0.029532	2.806097
150.715663	2583.600565	5.877760	-0.029606	2.810151
151.402642	2591.659971	5.882765	-0.029739	2.814239
151.813742	2599.684671	5.887770	-0.029821	2.818289
152.242117	2607.710438	5.892774	-0.029906	2.822333
152.600064	2615.752894	5.897779	-0.029978	2.826377
152.915676	2623.817536	5.902784	-0.030042	2.830423
153.181477	2631.918368	5.907789	-0.030096	2.834478
153.644876	2639.884903	5.912794	-0.030188	2.838472
153.687333	2647.956581	5.917798	-0.030201	2.842489
153.861634	2655.997710	5.922803	-0.030239	2.846492
154.268634	2664.026448	5.927808	-0.030320	2.850497
154.675652	2672.079954	5.932813	-0.030401	2.854508
155.067746	2680.100586	5.937818	-0.030479	2.858497
155.190119	2688.154152	5.942822	-0.030507	2.862481
155.506547	2696.183899	5.947827	-0.030571	2.866458
155.798977	2704.221328	5.952832	-0.030631	2.870432
156.053144	2712.318819	5.957837	-0.030683	2.874428
156.469965	2720.307118	5.962842	-0.030766	2.878374
156.951764	2728.338857	5.967846	-0.030861	2.882340
157.182989	2736.366465	5.972851	-0.030909	2.886284
157.533210	2744.408560	5.977856	-0.030980	2.890236
158.065547	2752.480663	5.982861	-0.031084	2.894207
157.981354	2760.535752	5.987866	-0.031074	2.898131
158.167181	2768.596223	5.992870	-0.031114	2.902067
158.566400	2776.621055	5.997875	-0.031193	2.905992
158.502538	2784.686784	6.002880	-0.031187	2.909906
158.799821	2792.827297	6.007885	-0.031247	2.913871
159.021163	2800.811988	6.012890	-0.031294	2.917750
159.290502	2808.811210	6.017894	-0.031349	2.921634
159.405624	2816.829056	6.022899	-0.031376	2.925514
159.720898	2824.803370	6.027904	-0.031440	2.929378
160.117451	2832.893636	6.032909	-0.031519	2.933297
160.272301	2840.927118	6.037914	-0.031553	2.937171
160.683332	2848.949305	6.042918	-0.031635	2.941048
160.929091	2856.967684	6.047923	-0.031685	2.944909
161.380346	2864.979687	6.052928	-0.031775	2.948772
161.587696	2873.077108	6.057933	-0.031819	2.952659
161.750535	2881.114962	6.062938	-0.031854	2.956509
162.028974	2889.145049	6.067942	-0.031911	2.960357
162.155386	2897.167355	6.072947	-0.031940	2.964189
162.487615	2905.192461	6.077952	-0.032007	2.968027
162.707034	2913.258618	6.082957	-0.032053	2.971874
162.738017	2921.296295	6.087962	-0.032064	2.975692
163.136768	2929.331417	6.092966	-0.032144	2.979524
163.443120	2937.365838	6.097971	-0.032206	2.983345
163.912537	2945.368297	6.102976	-0.032299	2.987155
164.308637	2953.449838	6.107981	-0.032378	2.990993
164.499724	2961.512056	6.112986	-0.032418	2.994807
164.905186	2969.519564	6.117990	-0.032499	2.998601
164.791300	2977.566366	6.122995	-0.032483	3.002382
165.199433	2985.533039	6.128000	-0.032564	3.006147
165.647138	2993.574962	6.133005	-0.032653	3.009945
165.513849	3001.686270	6.138010	-0.032633	3.013742
165.986815	3009.688856	6.143014	-0.032727	3.017512
166.221259	3017.725314	6.148019	-0.032776	3.021282
166.437549	3025.749758	6.153024	-0.032821	3.025041
166.680908	3033.798893	6.158029	-0.032872	3.028808
166.722394	3041.859733	6.163034	-0.032885	3.032566
166.993365	3049.905438	6.168038	-0.032940	3.036324
167.210149	3057.912429	6.173043	-0.032986	3.040056
167.245049	3065.931364	6.178048	-0.032998	3.043780
167.628068	3073.970031	6.183053	-0.033074	3.047525
167.761305	3082.010794	6.188058	-0.033104	3.051255
168.115063	3090.048929	6.193062	-0.033175	3.054990
168.354529	3098.091237	6.198067	-0.033225	3.058716
168.541868	3106.108875	6.203072	-0.033265	3.062424
168.872577	3114.152859	6.208077	-0.033332	3.066147
169.041006	3122.176522	6.213082	-0.033369	3.069847
169.215440	3130.329633	6.218086	-0.033406	3.073603
169.607726	3138.340714	6.223091	-0.033485	3.077300
169.966136	3146.322156	6.228096	-0.033557	3.080977
170.560230	3154.287410	6.233101	-0.033672	3.084653
170.769616	3162.312283	6.238106	-0.033717	3.088333
171.021141	3170.367205	6.243110	-0.033769	3.092026
171.216029	3178.436223	6.248115	-0.033810	3.095717
171.586289	3186.430197	6.253120	-0.033884	3.099378
172.072323	3194.460632	6.258125	-0.033980	3.103056
172.067545	3202.517001	6.263130	-0.033984	3.106720
172.367035	3210.554552	6.268134	-0.034045	3.110384
172.676040	3218.587022	6.273139	-0.034108	3.114042
172.711848	3226.619746	6.278144	-0.034120	3.117683
173.292655	3234.631231	6.283149	-0.034233	3.121335
173.648748	3242.597280	6.288154	-0.034305	3.124953
173.876199	3250.674022	6.293158	-0.034353	3.128610
174.135827	3258.741923	6.298163	-0.034406	3.132260
174.339083	3266.793030	6.303168	-0.034449	3.135896
174.617574	3274.823282	6.308173	-0.034506	3.139521
174.670248	3282.835081	6.313178	-0.034521	3.143125
174.914052	3290.872876	6.318182	-0.034572	3.146744
175.102664	3298.927539	6.323187	-0.034612	3.150364
175.200921	3306.988525	6.328192	-0.034636	3.153978
175.607255	3315.001590	6.333197	-0.034717	3.157581
175.907637	3323.016135	6.338202	-0.034778	3.161175
175.965876	3331.002552	6.343206	-0.034794	3.164742
176.275700	3339.051441	6.348211	-0.034857	3.168344
176.731283	3347.073128	6.353216	-0.034947	3.171936
177.110413	3355.133984	6.358221	-0.035023	3.175538
177.215414	3363.146891	6.363226	-0.035048	3.179103
177.305335	3371.190711	6.368230	-0.035070	3.182676
177.599767	3379.217690	6.373235	-0.035130	3.186247
177.870567	3387.244801	6.378240	-0.035185	3.189813
178.174207	3395.305445	6.383245	-0.035247	3.193391
178.434578	3403.325674	6.388250	-0.035301	3.196946
178.736989	3411.344600	6.393254	-0.035362	3.200497
178.608533	3419.377306	6.398259	-0.035344	3.204033
178.924442	3427.394514	6.403264	-0.035408	3.207576
179.194124	3435.467728	6.408269	-0.035463	3.211139
179.272860	3443.484857	6.413274	-0.035483	3.214664
179.620223	3451.516177	6.418278	-0.035553	3.218203
179.921428	3459.546597	6.423283	-0.035614	3.221736
179.973686	3467.568642	6.428288	-0.035629	3.225251
180.391076	3475.618905	6.433293	-0.035712	3.228790
180.542272	3483.682306	6.438298	-0.035746	3.232319
180.752353	3491.736955	6.443302	-0.035790	3.235843
181.015637	3499.699549	6.448307	-0.035844	3.239326
181.178106	3507.726809	6.453312	-0.035880	3.242828
181.661118	3515.737499	6.458317	-0.035975	3.246333
181.779515	3523.736827	6.463322	-0.036002	3.249814
182.078927	3531.815195	6.468326	-0.036063	3.253333
182.516962	3539.839300	6.473331	-0.036150	3.256829
182.532195	3547.848283	6.478336	-0.036158	3.260299
182.897553	3555.880697	6.483341	-0.036231	3.263789
183.086377	3563.896821	6.488346	-0.036271	3.267262
183.258500	3571.973012	6.493350	-0.036309	3.270755
183.528676	3580.009906	6.498355	-0.036364	3.274232
183.538033	3588.017519	6.503360	-0.036371	3.277683
183.819332	3596.057588	6.508365	-0.036429	3.281154
183.997234	3604.035737	6.513370	-0.036467	3.284591
184.464557	3612.060249	6.518374	-0.036559	3.288056
184.710771	3620.143198	6.523379	-0.036611	3.291533
184.726515	3628.174603	6.528384	-0.036619	3.294976
185.232034	3636.184423	6.533389	-0.036718	3.298424
185.384605	3644.203010	6.538394	-0.036752	3.301859
185.511422	3652.233056	6.543398	-0.036781	3.305295
185.628413	3660.300943	6.548403	-0.036808	3.308742
185.853695	3668.323734	6.553408	-0.036855	3.312171
186.690950	3676.330084	6.558413	-0.037016	3.315613
186.796493	3684.337883	6.563418	-0.037041	3.319024
187.031511	3692.378571	6.568422	-0.037090	3.322450
187.304369	3700.397863	6.573427	-0.037146	3.325864
187.223029	3708.416126	6.578432	-0.037136	3.329262
187.377260	3716.499322	6.583437	-0.037170	3.332693
187.561373	3724.532965	6.588442	-0.037209	3.336100
187.776870	3732.507168	6.593446	-0.037255	3.339479
187.907963	3740.587863	6.598451	-0.037284	3.342897
188.266725	3748.577181	6.603456	-0.037356	3.346281
188.640141	3756.623886	6.608461	-0.037431	3.349687
188.697275	3764.671440	6.613466	-0.037447	3.353078
189.008973	3772.694082	6.618470	-0.037510	3.356464
189.426698	3780.678693	6.623475	-0.037593	3.359834
189.526602	3788.703277	6.628480	-0.037617	3.363207
189.774997	3796.758256	6.633485	-0.037669	3.366594
189.939840	3804.780898	6.638490	-0.037704	3.369961
190.419664	3812.796733	6.643494	-0.037799	3.373333
190.680582	3820.847663	6.648499	-0.037853	3.376708
190.956360	3828.856164	6.653504	-0.037909	3.380063
191.343309	3836.883557	6.658509	-0.037987	3.383427
191.505025	3844.920173	6.663514	-0.038022	3.386783
191.407743	3852.968673	6.668518	-0.038009	3.390131
191.814022	3861.090860	6.673523	-0.038090	3.393524
191.830381	3869.096265	6.678528	-0.038098	3.396852
192.143588	3877.065880	6.683533	-0.038162	3.400172
192.380497	3885.052822	6.688538	-0.038211	3.403493
192.616303	3893.070388	6.693542	-0.038260	3.406824
193.045293	3901.088916	6.698547	-0.038345	3.410158
193.315703	3909.137713	6.703552	-0.038401	3.413496
193.659420	3917.170316	6.708557	-0.038470	3.416827
193.700186	3925.182199	6.713562	-0.038483	3.420135
193.879897	3933.219968	6.718566	-0.038522	3.423455
194.079124	3941.257962	6.723571	-0.038564	3.426774
194.365122	3949.258031	6.728576	-0.038623	3.430076
194.490386	3957.320114	6.733581	-0.038651	3.433395
194.706607	3965.375801	6.738586	-0.038697	3.436711
195.042859	3973.329138	6.743590	-0.038764	3.439986
195.204793	3981.385890	6.748595	-0.038800	3.443294
195.540619	3989.367756	6.753600	-0.038867	3.446575
195.694946	3997.427013	6.758605	-0.038901	3.449877
195.825728	4005.484508	6.763610	-0.038931	3.453175
196.012377	4013.504747	6.768614	-0.038971	3.456457
196.455671	4021.508294	6.773619	-0.039059	3.459737
196.763952	4029.492901	6.778624	-0.039121	3.463002
196.830901	4037.584223	6.783629	-0.039139	3.466299
197.192142	4045.587690	6.788634	-0.039212	3.469566
197.561281	4053.647434	6.793638	-0.039286	3.472854
197.677837	4061.727311	6.798643	-0.039313	3.476139
197.726934	4069.660844	6.803648	-0.039327	3.479359
198.144974	4077.697520	6.808653	-0.039410	3.482630
198.443919	4085.684976	6.813658	-0.039471	3.485873
198.432034	4093.736055	6.818662	-0.039474	3.489130
198.769803	4101.768846	6.823667	-0.039542	3.492387
198.885165	4109.808091	6.828672	-0.039569	3.495637
198.957924	4117.822578	6.833677	-0.039587	3.498872
199.141591	4125.826610	6.838682	-0.039627	3.502104
199.325309	4133.845880	6.843686	-0.039666	3.505338
199.624574	4141.906425	6.848691	-0.039727	3.508590
199.656255	4149.943148	6.853696	-0.039738	3.511821
200.118484	4157.978308	6.858701	-0.039830	3.515062
200.479460	4165.956457	6.863706	-0.039902	3.518273
200.512714	4174.003763	6.868710	-0.039914	3.521500
200.719006	4182.007049	6.873715	-0.039957	3.524711
200.742597	4190.049594	6.878720	-0.039967	3.527929
201.175593	4198.072333	6.883725	-0.040053	3.531149
201.222497	4206.093504	6.888730	-0.040067	3.534353
201.626885	4214.145876	6.893734	-0.040147	3.537578
201.805818	4222.185155	6.898739	-0.040186	3.540788
202.005843	4230.163565	6.903744	-0.040228	3.543971
202.680692	4238.192959	6.908749	-0.040359	3.547185
202.779300	4246.236086	6.913754	-0.040383	3.550385
202.855517	4254.377851	6.918758	-0.040402	3.553621
203.090703	4262.400328	6.923763	-0.040451	3.556811
203.364670	4270.312213	6.928768	-0.040507	3.559956
203.393963	4278.346317	6.933773	-0.040518	3.563139
203.313531	4286.389403	6.938778	-0.040508	3.566319
203.695108	4294.372471	6.943782	-0.040584	3.569486
203.879085	4302.426333	6.948787	-0.040624	3.572673
204.187207	4310.419034	6.953792	-0.040687	3.575836
204.398125	4318.429222	6.958797	-0.040731	3.579001
204.487105	4326.476091	6.963802	-0.040753	3.582173
204.683391	4334.478707	6.968806	-0.040795	3.585328
205.117578	4342.520490	6.973811	-0.040881	3.588503
205.371382	4350.553208	6.978816	-0.040933	3.591666
205.275469	4358.576937	6.983821	-0.040921	3.594813
205.246711	4366.590893	6.988826	-0.040920	3.597956
205.474964	4374.610977	6.993830	-0.040968	3.601105
205.916256	4382.606223	6.998835	-0.041055	3.604248
205.873457	4390.642336	7.003840	-0.041053	3.607390
206.077822	4398.687067	7.008845	-0.041096	3.610540
206.486364	4406.694063	7.013850	-0.041177	3.613678
206.670647	4414.701637	7.018854	-0.041217	3.616807
206.920787	4422.733230	7.023859	-0.041269	3.619944
207.132484	4430.752960	7.028864	-0.041313	3.623074
207.464423	4438.812237	7.033869	-0.041380	3.626219
207.625148	4446.828770	7.038874	-0.041416	3.629340
207.959126	4454.870767	7.043878	-0.041483	3.632473
208.356445	4462.925927	7.048883	-0.041562	3.635610
208.390981	4470.910263	7.053888	-0.041574	3.638707
208.723276	4478.938897	7.058893	-0.041641	3.641826
208.964123	4486.930846	7.063898	-0.041691	3.644926
209.021648	4494.960072	7.068902	-0.041707	3.648033
209.402027	4503.004775	7.073907	-0.041783	3.651152
209.699289	4511.031472	7.078912	-0.041844	3.654259
209.775362	4519.090730	7.083917	-0.041863	3.657370
209.791264	4527.080757	7.088922	-0.041871	3.660450
210.118945	4535.088044	7.093926	-0.041937	3.663543
210.473650	4543.128835	7.098931	-0.042009	3.666646
210.467865	4551.147256	7.103936	-0.042013	3.669729
210.754790	4559.189362	7.108941	-0.042071	3.672825
211.214784	4567.208090	7.113946	-0.042162	3.675915
211.317720	4575.178606	7.118950	-0.042187	3.678974
211.433901	4583.279642	7.123955	-0.042214	3.682081
211.634557	4591.242469	7.128960	-0.042256	3.685135
211.957304	4599.282304	7.133965	-0.042321	3.688218
211.887582	4607.360626	7.138970	-0.042314	3.691304
212.141866	4615.364670	7.143974	-0.042366	3.694367
212.551317	4623.389041	7.148979	-0.042448	3.697439
212.533371	4631.375304	7.153984	-0.042450	3.700484
212.682949	4639.369522	7.158989	-0.042483	3.703533
212.930195	4647.415750	7.163994	-0.042534	3.706601
212.980273	4655.428155	7.168998	-0.042548	3.709649
213.030273	4663.556506	7.174003	-0.042563	3.712739
213.349834	4671.548432	7.179008	-0.042628	3.715781
213.470453	4679.549126	7.184013	-0.042655	3.718819
213.646632	4687.547922	7.189018	-0.042693	3.721856
213.772961	4695.515282	7.194022	-0.042722	3.724876
214.307307	4703.544921	7.199027	-0.042827	3.727928
214.417593	4711.563674	7.204032	-0.042853	3.730962
214.398302	4719.616221	7.209037	-0.042854	3.734004
214.810614	4727.646468	7.214042	-0.042936	3.737045
215.055261	4735.619457	7.219046	-0.042987	3.740058
215.286998	4743.669413	7.224051	-0.043035	3.743097
215.707060	4751.656200	7.229056	-0.043119	3.746115
216.039159	4759.707390	7.234061	-0.043186	3.749152
216.114755	4767.786999	7.239066	-0.043205	3.752191
216.192202	4775.801579	7.244070	-0.043225	3.755204
216.433723	4783.825831	7.249075	-0.043275	3.758221
216.490168	4791.845538	7.254080	-0.043291	3.761230
216.677060	4799.811196	7.259085	-0.043331	3.764219
217.136080	4807.895107	7.264090	-0.043422	3.767257
217.227093	4815.903810	7.269094	-0.043444	3.770255
217.575908	4823.969289	7.274099	-0.043514	3.773278
217.966304	4831.981187	7.279104	-0.043592	3.776280
218.334021	4839.968369	7.284109	-0.043665	3.779269
218.543363	4848.046937	7.289114	-0.043710	3.782286
218.543417	4855.987859	7.294118	-0.043715	3.785245
218.784680	4864.063196	7.299123	-0.043765	3.788257
219.066076	4872.049499	7.304128	-0.043823	3.791235
219.249013	4880.142150	7.309133	-0.043862	3.794247
219.430143	4888.144732	7.314138	-0.043901	3.797224
219.637982	4896.099090	7.319142	-0.043945	3.800181
220.004170	4904.111072	7.324147	-0.044018	3.803160
219.894980	4912.118570	7.329152	-0.044003	3.806125
220.343099	4920.165537	7.334157	-0.044092	3.809114
220.549693	4928.190870	7.339162	-0.044135	3.812088
220.633226	4936.211114	7.344166	-0.044156	3.815055
221.026107	4944.231609	7.349171	-0.044235	3.818026
221.124768	4952.240778	7.354176	-0.044258	3.820984
221.348939	4960.214284	7.359181	-0.044305	3.823930
221.663713	4968.312589	7.364186	-0.044369	3.826921
221.916572	4976.278419	7.369190	-0.044421	3.829860
222.143427	4984.383522	7.374195	-0.044469	3.832847
222.174085	4992.382989	7.379200	-0.044480	3.835789
222.386182	5000.355430	7.384205	-0.044524	3.838722
222.712354	5008.408477	7.389210	-0.044590	3.841686
222.761250	5016.361671	7.394214	-0.044605	3.844604
223.082171	5024.440376	7.399219	-0.044670	3.847572
223.332094	5032.444142	7.404224	-0.044721	3.850508
223.446440	5040.515412	7.409229	-0.044748	3.853465
223.684233	5048.541707	7.414234	-0.044798	3.856405
223.971334	5056.507421	7.419238	-0.044856	3.859321
224.078600	5064.580677	7.424243	-0.044881	3.862271
224.138565	5072.537768	7.429248	-0.044898	3.865175
224.504294	5080.621289	7.434253	-0.044971	3.868130
224.585064	5088.682038	7.439258	-0.044991	3.871068
224.818753	5096.900270	7.444262	-0.045040	3.874064
224.978615	5104.856762	7.449267	-0.045075	3.876961
225.197951	5112.767108	7.454272	-0.045121	3.879841
225.219869	5120.763644	7.459277	-0.045130	3.882745
225.440297	5128.751303	7.464282	-0.045177	3.885649
225.460700	5136.753935	7.469286	-0.045186	3.888551
225.679688	5144.801183	7.474291	-0.045232	3.891471
225.677457	5152.833462	7.479296	-0.045237	3.894380
225.977687	5160.828247	7.484301	-0.045298	3.897278
226.300242	5168.836590	7.489306	-0.045363	3.900180
226.456007	5176.840717	7.494310	-0.045397	3.903075
226.862385	5184.844767	7.499315	-0.045478	3.905972
226.940949	5192.862377	7.504320	-0.045498	3.908866
227.087890	5200.924898	7.509325	-0.045530	3.911775
227.175179	5208.972277	7.514330	-0.045552	3.914675
227.475125	5216.928022	7.519334	-0.045613	3.917544
227.958503	5224.946380	7.524339	-0.045708	3.920437
228.064014	5232.959641	7.529344	-0.045733	3.923319
228.449436	5240.985564	7.534349	-0.045810	3.926208
228.664178	5249.018335	7.539354	-0.045855	3.929095
228.777988	5257.063048	7.544358	-0.045882	3.931982
229.072760	5265.097712	7.549363	-0.045942	3.934866
229.089973	5273.091169	7.554368	-0.045950	3.937729
229.425306	5281.093883	7.559373	-0.046018	3.940598
229.461096	5289.124364	7.564378	-0.046030	3.943470
229.629350	5297.130603	7.569382	-0.046066	3.946334
230.080757	5305.166474	7.574387	-0.046156	3.949211
230.047456	5313.205801	7.579392	-0.046155	3.952078
230.108267	5321.265658	7.584397	-0.046171	3.954953
230.337350	5329.265403	7.589402	-0.046219	3.957807
230.473654	5337.215843	7.594406	-0.046250	3.960639
230.549177	5345.256607	7.599411	-0.046269	3.963501
230.821225	5353.234077	7.604416	-0.046325	3.966341
231.128456	5361.264068	7.609421	-0.046387	3.969199
231.257744	5369.348021	7.614426	-0.046417	3.972070
231.267802	5377.357231	7.619430	-0.046424	3.974911
231.677710	5385.370989	7.624435	-0.046505	3.977759
231.606250	5393.347095	7.629440	-0.046497	3.980582
231.946169	5401.379352	7.634445	-0.046566	3.983431
232.148791	5409.416827	7.639450	-0.046609	3.986277
232.204524	5417.437775	7.644454	-0.046624	3.989113
232.272288	5425.479825	7.649459	-0.046642	3.991954
232.455039	5433.535637	7.654464	-0.046681	3.994800
232.897952	5441.535800	7.659469	-0.046769	3.997629
233.177542	5449.559002	7.664474	-0.046826	4.000461
233.251886	5457.554744	7.669478	-0.046845	4.003278
233.394787	5465.596550	7.674483	-0.046877	4.006110
233.558390	5473.569473	7.679488	-0.046913	4.008916
233.945615	5481.634040	7.684493	-0.046990	4.011756
234.174113	5489.681323	7.689498	-0.047038	4.014586
234.055110	5497.692830	7.694502	-0.047021	4.017395
234.262410	5505.703518	7.699507	-0.047065	4.020208
234.465912	5513.706707	7.704512	-0.047108	4.023015
234.738622	5521.719687	7.709517	-0.047164	4.025825
234.999536	5529.756752	7.714522	-0.047218	4.028642
235.015915	5537.756571	7.719526	-0.047226	4.031439
235.454793	5545.906392	7.724531	-0.047313	4.034294
235.626906	5553.858089	7.729536	-0.047350	4.037073
235.756030	5561.809127	7.734541	-0.047379	4.039849
236.175688	5569.836621	7.739546	-0.047463	4.042655
236.165813	5577.829820	7.744550	-0.047466	4.045440
236.248335	5585.876653	7.749555	-0.047487	4.048243
236.395688	5593.881507	7.754560	-0.047519	4.051031
236.660560	5601.925651	7.759565	-0.047574	4.053832
236.961837	5609.935317	7.764570	-0.047635	4.056619
236.757752	5617.913991	7.769574	-0.047603	4.059387
237.043793	5625.957931	7.774579	-0.047661	4.062183
237.145782	5633.952046	7.779584	-0.047685	4.064956
237.404667	5641.977710	7.784589	-0.047739	4.067741
237.848162	5650.005998	7.789594	-0.047826	4.070527
237.973296	5658.026680	7.794598	-0.047855	4.073305
238.431738	5666.081028	7.799603	-0.047946	4.076096
238.366659	5674.045477	7.804608	-0.047939	4.078848
238.663938	5682.059628	7.809613	-0.047999	4.081620
238.748545	5690.049782	7.814618	-0.048020	4.084378
238.839302	5698.116677	7.819622	-0.048042	4.087161
239.087515	5706.107721	7.824627	-0.048094	4.089919
239.327427	5714.127262	7.829632	-0.048144	4.092684
239.537390	5722.170739	7.834637	-0.048188	4.095455
239.493662	5730.225031	7.839642	-0.048185	4.098225
239.512498	5738.181491	7.844646	-0.048194	4.100959
239.704766	5746.205741	7.849651	-0.048235	4.103718
239.774624	5754.262888	7.854656	-0.048253	4.106484
239.970344	5762.288867	7.859661	-0.048295	4.109240
240.362864	5770.360280	7.864666	-0.048373	4.112012
240.559766	5778.362591	7.869670	-0.048415	4.114755
240.609961	5786.424160	7.874675	-0.048430	4.117515
240.831929	5794.346020	7.879680	-0.048476	4.120228
241.200867	5802.350907	7.884685	-0.048550	4.122969
241.124227	5810.392274	7.889690	-0.048541	4.125715
241.359042	5818.401066	7.894694	-0.048590	4.128452
241.520218	5826.453655	7.899699	-0.048625	4.131202
241.679640	5834.483349	7.904704	-0.048660	4.133941
241.902797	5842.544568	7.909709	-0.048707	4.136690
242.130259	5850.535880	7.914714	-0.048754	4.139414
242.340710	5858.514804	7.919718	-0.048799	4.142131
242.555796	5866.509001	7.924723	-0.048844	4.144852
242.677755	5874.576158	7.929728	-0.048872	4.147595
242.736249	5882.579196	7.934733	-0.048888	4.150313
243.023274	5890.626499	7.939738	-0.048947	4.153048
243.243473	5898.634576	7.944742	-0.048993	4.155766
243.506483	5906.649287	7.949747	-0.049047	4.158485
243.590088	5914.648753	7.954752	-0.049068	4.161195
243.731241	5922.628451	7.959757	-0.049099	4.163898
243.956769	5930.715806	7.964762	-0.049147	4.166636
243.933050	5938.652497	7.969766	-0.049147	4.169318
244.235759	5946.732239	7.974771	-0.049209	4.172051
244.425202	5954.799895	7.979776	-0.049250	4.174776
244.614836	5962.768291	7.984781	-0.049290	4.177467
244.743949	5970.767056	7.989786	-0.049319	4.180165
245.120386	5978.762975	7.994790	-0.049395	4.182863
245.180324	5986.787474	7.999795	-0.049411	4.185565
245.375158	5994.804487	8.004800	-0.049452	4.188265
245.439067	6002.855104	8.009805	-0.049470	4.190972
245.729183	6010.984612	8.014810	-0.049529	4.193707
245.741627	6018.986057	8.019814	-0.049536	4.196394
246.163756	6026.913679	8.024819	-0.049620	4.199059
246.172603	6034.924624	8.029824	-0.049627	4.201746
246.401665	6042.863048	8.034829	-0.049675	4.204409
246.299662	6050.920325	8.039834	-0.049661	4.207107
246.465940	6058.847621	8.044838	-0.049697	4.209762
246.887331	6066.963598	8.049843	-0.049781	4.212481
246.876882	6075.000931	8.054848	-0.049784	4.215168
247.138124	6083.011846	8.059853	-0.049838	4.217847
247.444276	6091.050945	8.064858	-0.049900	4.220534
247.669531	6099.029377	8.069862	-0.049948	4.223199
247.943626	6107.028363	8.074867	-0.050004	4.225869
248.120205	6115.081309	8.079872	-0.050042	4.228554
248.193969	6123.092746	8.084877	-0.050061	4.231222
248.200510	6131.178787	8.089882	-0.050067	4.233914
248.546639	6139.128766	8.094886	-0.050137	4.236561
248.798268	6147.109113	8.099891	-0.050189	4.239216
248.709541	6155.160632	8.104896	-0.050178	4.241890
249.044520	6163.130011	8.109901	-0.050245	4.244538
249.636816	6171.227224	8.114906	-0.050361	4.247230
249.672064	6179.172912	8.119910	-0.050373	4.249865
249.705770	6187.289483	8.124915	-0.050384	4.252555
249.913901	6195.287602	8.129920	-0.050428	4.255205
250.222899	6203.299383	8.134925	-0.050491	4.257859
250.304919	6211.302590	8.139930	-0.050511	4.260506
250.733909	6219.291126	8.144934	-0.050596	4.263150
250.722420	6227.356085	8.149939	-0.050600	4.265814
250.723102	6235.409683	8.154944	-0.050605	4.268472
251.093480	6243.392352	8.159949	-0.050679	4.271109
251.511776	6251.494436	8.164954	-0.050762	4.273784
251.551365	6259.479791	8.169958	-0.050775	4.276415
251.541055	6267.440067	8.174963	-0.050778	4.279036
251.870958	6275.497176	8.179968	-0.050845	4.281690
252.067018	6283.418455	8.184973	-0.050886	4.284296
252.087125	6291.505839	8.189978	-0.050895	4.286954
252.234412	6299.469589	8.194982	-0.050928	4.289571
252.527911	6307.545981	8.199987	-0.050988	4.292225
252.768705	6315.583090	8.204992	-0.051038	4.294863
252.898771	6323.579349	8.209997	-0.051067	4.297485
253.277653	6331.609834	8.215002	-0.051143	4.300119
253.193261	6339.590649	8.220006	-0.051133	4.302732
253.622480	6347.618528	8.225011	-0.051218	4.305362
253.684687	6355.623825	8.230016	-0.051235	4.307981
253.865427	6363.633177	8.235021	-0.051274	4.310600
254.180133	6371.713229	8.240026	-0.051337	4.313241
254.414355	6379.704540	8.245030	-0.051386	4.315852
254.622972	6387.683182	8.250035	-0.051430	4.318456
254.644206	6395.725549	8.255040	-0.051439	4.321078
254.880562	6403.676005	8.260045	-0.051489	4.323670
255.093696	6411.756524	8.265050	-0.051534	4.326303
255.182543	6419.740183	8.270054	-0.051555	4.328902
255.130685	6427.797035	8.275059	-0.051551	4.331522
255.473705	6435.849289	8.280064	-0.051620	4.334142
255.674573	6443.841334	8.285069	-0.051663	4.336739
255.943153	6451.791615	8.290074	-0.051718	4.339322
255.964494	6459.855882	8.295078	-0.051727	4.341938
256.237921	6467.836006	8.300083	-0.051783	4.344528
256.330633	6475.875800	8.305088	-0.051806	4.347134
256.487049	6483.866129	8.310093	-0.051840	4.349722
256.860599	6491.967871	8.315098	-0.051915	4.352347
256.919231	6500.006610	8.320102	-0.051931	4.354948
257.087376	6508.006480	8.325107	-0.051967	4.357535
257.155625	6515.969637	8.330112	-0.051985	4.360108
257.712451	6523.954176	8.335117	-0.052094	4.362690
257.791432	6531.942199	8.340122	-0.052114	4.365268
258.025387	6539.987236	8.345126	-0.052163	4.367864
258.160736	6548.023511	8.350131	-0.052193	4.370455
258.213454	6556.052581	8.355136	-0.052208	4.373041
258.318993	6564.072850	8.360141	-0.052233	4.375624
258.621768	6572.118582	8.365146	-0.052295	4.378214
258.819633	6580.063289	8.370150	-0.052337	4.380770
259.082372	6588.102916	8.375155	-0.052391	4.383355
259.211885	6596.070013	8.380160	-0.052420	4.385914
259.501387	6604.143143	8.385165	-0.052480	4.388507
259.589712	6612.178882	8.390170	-0.052501	4.391085
259.743213	6620.186129	8.395174	-0.052535	4.393653
259.992068	6628.217966	8.400179	-0.052587	4.396228
259.981429	6636.242361	8.405184	-0.052590	4.398797
260.075050	6644.239483	8.410189	-0.052612	4.401357
260.338343	6652.203394	8.415194	-0.052667	4.403905
260.322006	6660.253708	8.420198	-0.052669	4.406479
260.516367	6668.271168	8.425203	-0.052710	4.409041
260.806699	6676.324150	8.430208	-0.052770	4.411613
261.056179	6684.342463	8.435213	-0.052821	4.414173
261.262829	6692.419073	8.440218	-0.052865	4.416750
261.180403	6700.369632	8.445222	-0.052855	4.419283
261.620021	6708.367931	8.450227	-0.052942	4.421833
261.821286	6716.381401	8.455232	-0.052985	4.424385
261.753393	6724.416252	8.460237	-0.052977	4.426941
261.991899	6732.470983	8.465242	-0.053027	4.429503
262.098365	6740.473383	8.470246	-0.053052	4.432047
262.311780	6748.540887	8.475251	-0.053097	4.434610
262.509619	6756.560237	8.480256	-0.053139	4.437156
262.598881	6764.425287	8.485261	-0.053161	4.439651
262.874906	6772.509010	8.490266	-0.053217	4.442216
263.005698	6780.499888	8.495270	-0.053247	4.444748
263.242033	6788.561073	8.500275	-0.053296	4.447302
263.540659	6796.579824	8.505280	-0.053357	4.449841
263.591541	6804.579737	8.510285	-0.053372	4.452372
263.751433	6812.647091	8.515290	-0.053407	4.454923
263.868859	6820.654422	8.520294	-0.053434	4.457453
264.088337	6828.621620	8.525299	-0.053480	4.459970
264.199906	6836.662961	8.530304	-0.053506	4.462508
264.395215	6844.604002	8.535309	-0.053547	4.465013
264.503480	6852.691253	8.540314	-0.053573	4.467563
264.601042	6860.700032	8.545318	-0.053596	4.470087
264.726906	6868.751751	8.550323	-0.053625	4.472622
265.076411	6876.769954	8.555328	-0.053695	4.475147
265.136420	6884.759165	8.560333	-0.053712	4.477660
265.252225	6892.788080	8.565338	-0.053738	4.480184
265.718884	6900.755363	8.570343	-0.053830	4.482688
265.658217	6908.761426	8.575347	-0.053824	4.485202
265.827612	6916.793585	8.580352	-0.053861	4.487723
266.121643	6924.785322	8.585357	-0.053921	4.490230
266.155558	6932.879751	8.590362	-0.053933	4.492767
266.414488	6940.855078	8.595367	-0.053986	4.495267
266.471676	6948.864707	8.600371	-0.054002	4.497774
266.590258	6956.863323	8.605376	-0.054029	4.500278
266.688722	6964.891584	8.610381	-0.054053	4.502789
266.868989	6972.878721	8.615386	-0.054092	4.505286
267.012118	6980.922657	8.620391	-0.054123	4.507799
267.032360	6988.949135	8.625395	-0.054132	4.510305
267.423116	6997.060237	8.630400	-0.054210	4.512837
267.590947	7005.067620	8.635405	-0.054247	4.515334
267.912150	7013.043294	8.640410	-0.054312	4.517821
268.010090	7021.004074	8.645415	-0.054335	4.520301
268.326555	7028.985773	8.650419	-0.054399	4.522787
268.556752	7036.981624	8.655424	-0.054448	4.525276
268.514815	7045.041039	8.660429	-0.054445	4.527782
268.641911	7053.084719	8.665434	-0.054474	4.530282
268.974461	7061.089379	8.670439	-0.054541	4.532770
269.213882	7069.092104	8.675443	-0.054591	4.535255
269.368053	7077.140083	8.680448	-0.054625	4.537752
269.386047	7085.082581	8.685453	-0.054633	4.540216
269.790224	7093.154210	8.690458	-0.054714	4.542718
270.899110	7101.098663	8.695463	-0.054925	4.545181
271.442462	7109.189976	8.700467	-0.055032	4.547687
271.985639	7117.166889	8.705472	-0.055138	4.550156
272.274853	7125.195004	8.710477	-0.055197	4.552640
272.442079	7133.255458	8.715482	-0.055234	4.555131
272.551953	7141.234725	8.720487	-0.055259	4.557596
272.872544	7149.242769	8.725491	-0.055324	4.560069
272.807082	7157.294272	8.730496	-0.055317	4.562554
272.994022	7165.261101	8.735501	-0.055357	4.565011
273.212240	7173.311211	8.740506	-0.055403	4.567493
273.457889	7181.316032	8.745511	-0.055454	4.569959
273.406375	7189.387082	8.750515	-0.055450	4.572444
273.648638	7197.393641	8.755520	-0.055500	4.574908
273.848782	7205.345849	8.760525	-0.055543	4.577355
273.923909	7213.424626	8.765530	-0.055562	4.579838
274.145884	7221.411928	8.770535	-0.055608	4.582292
274.152894	7229.416288	8.775539	-0.055615	4.584750
274.177385	7237.485968	8.780544	-0.055625	4.587227
274.396890	7245.535237	8.785549	-0.055671	4.589696
274.892131	7253.554868	8.790554	-0.055768	4.592155
274.914803	7261.508338	8.795559	-0.055778	4.594592
274.765539	7269.565174	8.800563	-0.055755	4.597059
274.795214	7277.508770	8.805568	-0.055766	4.599491
274.977525	7285.525871	8.810573	-0.055805	4.601943
275.334011	7293.510443	8.815578	-0.055876	4.604385
275.397515	7301.579246	8.820583	-0.055894	4.606851
275.612075	7309.581813	8.825587	-0.055939	4.609295
275.538257	7317.632732	8.830592	-0.055930	4.611753
275.580803	7325.649044	8.835597	-0.055943	4.614198
276.021635	7333.697406	8.840602	-0.056031	4.616652
275.884595	7341.607515	8.845607	-0.056010	4.619063
275.996815	7349.672585	8.850611	-0.056036	4.621520
276.242717	7357.694934	8.855616	-0.056087	4.623962
276.293824	7365.668050	8.860621	-0.056102	4.626388
276.520267	7373.695917	8.865626	-0.056150	4.628830
276.654643	7381.725928	8.870631	-0.056180	4.631271
276.824833	7389.777769	8.875635	-0.056217	4.633717
277.017098	7397.840151	8.880640	-0.056258	4.636165
276.934447	7405.742700	8.885645	-0.056248	4.638563
277.315015	7413.830527	8.890650	-0.056324	4.641016
277.351166	7421.795243	8.895655	-0.056336	4.643431
277.433753	7429.785894	8.900659	-0.056356	4.645852
277.660223	7437.851280	8.905664	-0.056404	4.648294
277.787308	7445.801023	8.910669	-0.056432	4.650700
278.045413	7453.907105	8.915674	-0.056486	4.653152
278.117248	7461.871308	8.920679	-0.056504	4.655560
278.301905	7469.891744	8.925683	-0.056544	4.657984
278.627224	7477.896296	8.930688	-0.056610	4.660401
278.591803	7485.920243	8.935693	-0.056608	4.662823
278.817283	7493.939103	8.940698	-0.056656	4.665243
278.824736	7501.929161	8.945703	-0.056662	4.667652
279.005558	7509.974921	8.950707	-0.056701	4.670077
279.259790	7518.087488	8.955712	-0.056754	4.672521
279.416447	7526.113691	8.960717	-0.056788	4.674937
279.557092	7534.096299	8.965722	-0.056819	4.677339
279.637379	7542.025646	8.970727	-0.056840	4.679724
279.902098	7550.016195	8.975731	-0.056894	4.682126
280.157521	7558.012982	8.980736	-0.056947	4.684528
280.343548	7566.068678	8.985741	-0.056987	4.686947
280.540685	7574.071464	8.990746	-0.057029	4.689349
280.514005	7582.090548	8.995751	-0.057029	4.691755
280.680874	7590.110845	9.000755	-0.057065	4.694159
280.856910	7598.191657	9.005760	-0.057103	4.696581
281.004989	7606.101376	9.010765	-0.057136	4.698950
281.313773	7614.151894	9.015770	-0.057199	4.701359
281.125151	7622.166501	9.020775	-0.057169	4.703758
281.477903	7630.185027	9.025779	-0.057240	4.706155
281.800957	7638.230540	9.030784	-0.057305	4.708560
281.630798	7646.254448	9.035789	-0.057279	4.710957
281.944115	7654.312447	9.040794	-0.057342	4.713363
282.061010	7662.239136	9.045799	-0.057369	4.715728
282.324763	7670.273694	9.050803	-0.057423	4.718124
282.443311	7678.267194	9.055808	-0.057451	4.720507
282.506661	7686.245435	9.060813	-0.057468	4.722885
282.690914	7694.306409	9.065818	-0.057507	4.725285
282.918298	7702.342590	9.070823	-0.057555	4.727677
283.054149	7710.340090	9.075827	-0.057585	4.730056
283.345415	7718.395679	9.080832	-0.057645	4.732451
283.278726	7726.363694	9.085837	-0.057638	4.734820
283.614057	7734.426962	9.090842	-0.057705	4.737215
283.809757	7742.391007	9.095847	-0.057747	4.739579
284.052390	7750.501646	9.100851	-0.057797	4.741985
284.063996	7758.487723	9.105856	-0.057805	4.744354
284.168454	7766.472490	9.110861	-0.057829	4.746721
284.637056	7774.475843	9.115866	-0.057922	4.749092
284.588295	7782.553487	9.120871	-0.057918	4.751484
284.823319	7790.540332	9.125875	-0.057967	4.753848
284.858700	7798.597531	9.130880	-0.057979	4.756232
285.064675	7806.507702	9.135885	-0.058022	4.758571
285.482947	7814.601878	9.140890	-0.058106	4.760962
285.417586	7822.556989	9.145895	-0.058099	4.763312
285.318665	7830.534630	9.150899	-0.058085	4.765668
285.540388	7838.623910	9.155904	-0.058132	4.768055
285.837674	7846.598686	9.160909	-0.058192	4.770407
286.217471	7854.697206	9.165914	-0.058268	4.772793
286.150767	7862.624515	9.170919	-0.058261	4.775130
286.393558	7870.712484	9.175923	-0.058312	4.777511
286.706549	7878.661291	9.180928	-0.058375	4.779850
286.739157	7886.732299	9.185933	-0.058386	4.782225
286.826627	7894.667957	9.190938	-0.058408	4.784559
286.943109	7902.727976	9.195943	-0.058435	4.786928
287.130831	7910.733545	9.200947	-0.058475	4.789279
287.456242	7918.764269	9.205952	-0.058541	4.791636
287.531184	7926.813476	9.210957	-0.058560	4.793999
287.941673	7934.833382	9.215962	-0.058642	4.796350
287.890462	7942.765214	9.220967	-0.058637	4.798676
287.985582	7950.753199	9.225971	-0.058660	4.801017
288.328965	7958.821460	9.230976	-0.058729	4.803379
288.434861	7966.791988	9.235981	-0.058754	4.805713
288.606046	7974.918989	9.240986	-0.058791	4.808090
288.624881	7982.845872	9.245991	-0.058800	4.810409
288.759494	7990.351269	9.250995	-0.058830	4.812603
289.143492	7995.056435	9.256000	-0.058905	4.813976
289.141825	7997.605643	9.261005	-0.058906	4.814721
289.364447	7998.940714	9.266010	-0.058948	4.815110
289.284377	7999.316609	9.271015	-0.058934	4.815220
289.291092	8000.481548	9.276019	-0.058936	4.815561
289.642019	8000.465973	9.281024	-0.059001	4.815554
289.529790	8000.456637	9.286029	-0.058980	4.815552
289.831306	8000.433833	9.291034	-0.059036	4.815544
289.889648	8000.426248	9.296039	-0.059047	4.815542
290.033504	8000.455342	9.301043	-0.059074	4.815549
290.007639	8000.486976	9.306048	-0.059069	4.815559
289.991264	8000.456781	9.311053	-0.059066	4.815550
289.980259	8000.479041	9.316058	-0.059064	4.815557
289.880159	8000.469905	9.321063	-0.059045	4.815554
289.986951	8000.482357	9.326067	-0.059065	4.815557
290.384478	8000.483585	9.331072	-0.059139	4.815556
290.290497	8000.470275	9.336077	-0.059122	4.815552
290.266630	8000.484842	9.341082	-0.059117	4.815557
290.374859	8000.490905	9.346087	-0.059137	4.815558
290.352863	8000.509778	9.351091	-0.059133	4.815564
290.388676	8000.509301	9.356096	-0.059140	4.815563
290.493536	8000.482179	9.361101	-0.059159	4.815555
290.738407	8000.520426	9.366106	-0.059205	4.815565
290.693227	8000.494029	9.371111	-0.059197	4.815557
290.803862	8000.501202	9.376115	-0.059217	4.815559
290.853132	8000.510566	9.381120	-0.059226	4.815562
290.851881	8000.485964	9.386125	-0.059226	4.815554
290.513581	8000.530600	9.391130	-0.059163	4.815569
290.612281	8000.504445	9.396135	-0.059182	4.815561
290.877398	8000.514172	9.401139	-0.059231	4.815562
290.846488	8000.482667	9.406144	-0.059225	4.815553
290.715016	8000.454844	9.411149	-0.059201	4.815546
290.794764	8000.491430	9.416154	-0.059215	4.815556
290.744165	8000.478837	9.421159	-0.059206	4.815553
290.711571	8000.464404	9.426163	-0.059200	4.815549
291.003244	8000.521594	9.431168	-0.059254	4.815564
290.965572	8000.468603	9.436173	-0.059247	4.815549
291.025706	8000.525171	9.441178	-0.059258	4.815565
291.009721	8000.473607	9.446183	-0.059255	4.815550
290.951079	8000.475843	9.451187	-0.059245	4.815551
290.867652	8000.493701	9.456192	-0.059229	4.815557
290.978627	8000.478436	9.461197	-0.059250	4.815552
291.184585	8000.526728	9.466202	-0.059288	4.815565
290.954710	8000.506895	9.471207	-0.059245	4.815560
290.849662	8000.504089	9.476211	-0.059226	4.815560
291.001505	8000.482018	9.481216	-0.059254	4.815552
290.980841	8000.472058	9.486221	-0.059250	4.815550
291.037293	8000.510396	9.491226	-0.059261	4.815561
291.071168	8000.487444	9.496231	-0.059267	4.815554
290.960862	8000.504857	9.501235	-0.059246	4.815559
291.021416	8000.509064	9.506240	-0.059258	4.815560
290.955002	8000.479110	9.511245	-0.059245	4.815552
291.341063	8000.485493	9.516250	-0.059317	4.815552
291.289532	8000.469679	9.521255	-0.059307	4.815547
291.070977	8000.478889	9.526259	-0.059267	4.815551
291.024297	8000.514453	9.531264	-0.059258	4.815562
291.096040	8000.472890	9.536269	-0.059271	4.815549
291.122729	8000.519286	9.541274	-0.059276	4.815563
291.036798	8000.489009	9.546279	-0.059260	4.815554
291.108819	8000.473100	9.551283	-0.059274	4.815549
291.209289	8000.495067	9.556288	-0.059293	4.815555
291.090346	8000.487756	9.561293	-0.059270	4.815554
291.524789	8000.503491	9.566298	-0.059351	4.815556
291.490342	8000.494370	9.571303	-0.059345	4.815554
291.399819	8000.473635	9.576307	-0.059328	4.815548
291.557761	8000.490141	9.581312	-0.059357	4.815552
291.343545	8000.457742	9.586317	-0.059317	4.815544
291.360268	8000.507180	9.591322	-0.059321	4.815558
291.216123	8000.484489	9.596327	-0.059294	4.815552
291.204093	8000.492840	9.601331	-0.059292	4.815555
291.343399	8000.512243	9.606336	-0.059317	4.815560
291.482846	8000.461112	9.611341	-0.059343	4.815544
291.632174	8000.506331	9.616346	-0.059371	4.815557
291.708513	8000.476600	9.621351	-0.059385	4.815547
291.663977	8000.498307	9.626355	-0.059377	4.815554
291.627157	8000.508385	9.631360	-0.059370	4.815557
291.347946	8000.497354	9.636365	-0.059318	4.815555
291.340055	8000.513254	9.641370	-0.059317	4.815560
291.315560	8000.490405	9.646375	-0.059312	4.815553
291.452361	8000.491598	9.651379	-0.059338	4.815553
291.482808	8000.519889	9.656384	-0.059343	4.815561
291.310285	8000.498866	9.661389	-0.059311	4.815556
291.338950	8000.586977	9.666394	-0.059317	4.815582
291.311576	8000.450794	9.671399	-0.059311	4.815542
291.204392	8000.527038	9.676403	-0.059292	4.815565
291.410742	8000.537932	9.681408	-0.059330	4.815567
291.408851	8000.494082	9.686413	-0.059330	4.815554
291.337668	8000.523898	9.691418	-0.059316	4.815563
291.361932	8000.484755	9.696423	-0.059321	4.815552
291.430835	8000.498719	9.701427	-0.059334	4.815555
291.531186	8000.524960	9.706432	-0.059352	4.815562
291.457481	8000.459616	9.711437	-0.059339	4.815544
291.375255	8000.471080	9.716442	-0.059323	4.815547
291.465681	8000.511050	9.721447	-0.059340	4.815559
291.441084	8000.502093	9.726451	-0.059336	4.815556
291.467036	8000.527103	9.731456	-0.059340	4.815563
291.441133	8000.494612	9.736461	-0.059336	4.815554
291.343125	8000.531465	9.741466	-0.059317	4.815565
291.434176	8000.497702	9.746471	-0.059334	4.815555
291.506013	8000.489271	9.751475	-0.059348	4.815552
291.649989	8000.506615	9.756480	-0.059374	4.815557
291.346703	8000.472742	9.761485	-0.059318	4.815548
291.311328	8000.534144	9.766490	-0.059311	4.815566
291.535343	8000.498305	9.771495	-0.059353	4.815555
291.432859	8000.489128	9.776499	-0.059334	4.815552
291.432640	8000.491262	9.781504	-0.059334	4.815553
291.450520	8000.472320	9.786509	-0.059337	4.815547
291.589522	8000.510956	9.791514	-0.059363	4.815558
291.427777	8000.501867	9.796519	-0.059333	4.815556
291.363331	8000.478358	9.801523	-0.059321	4.815550
291.627520	8000.506239	9.806528	-0.059370	4.815557
291.656343	8000.459691	9.811533	-0.059376	4.815543
291.819319	8000.520098	9.816538	-0.059406	4.815560
291.762294	8000.509536	9.821543	-0.059395	4.815557
291.695389	8000.477435	9.826547	-0.059383	4.815548
291.816102	8000.516838	9.831552	-0.059405	4.815559
291.770963	8000.508609	9.836557	-0.059397	4.815557
291.741681	8000.513468	9.841562	-0.059391	4.815558
291.685539	8000.505058	9.846567	-0.059381	4.815556
291.511572	8000.507524	9.851571	-0.059349	4.815557
291.758677	8000.528711	9.856576	-0.059395	4.815562
291.682731	8000.490048	9.861581	-0.059380	4.815552
291.640432	8000.523548	9.866586	-0.059373	4.815562
291.623758	8000.518997	9.871591	-0.059369	4.815560
291.713720	8000.474528	9.876595	-0.059386	4.815547
291.779113	8000.510878	9.881600	-0.059398	4.815557
291.795540	8000.510081	9.886605	-0.059401	4.815557
291.989964	8000.545359	9.891610	-0.059438	4.815566
291.817108	8000.507230	9.896615	-0.059405	4.815556
291.684980	8000.516801	9.901619	-0.059381	4.815559
291.737189	8000.502701	9.906624	-0.059390	4.815555
291.698689	8000.431527	9.911629	-0.059383	4.815534
291.595427	8000.427681	9.916634	-0.059364	4.815534
291.822162	8000.497693	9.921639	-0.059406	4.815553
291.771200	8000.446619	9.926643	-0.059397	4.815538
291.714392	8000.508735	9.931648	-0.059386	4.815557
291.850082	8000.468229	9.936653	-0.059411	4.815544
292.142576	8000.523299	9.941658	-0.059466	4.815559
292.083814	8000.529807	9.946663	-0.059455	4.815561
291.833805	8000.498952	9.951667	-0.059408	4.815553
292.053235	8000.530370	9.956672	-0.059449	4.815562
292.152493	8000.509567	9.961677	-0.059468	4.815555
292.023416	8000.523463	9.966682	-0.059444	4.815560
292.054046	8000.529313	9.971687	-0.059449	4.815561
292.145437	8000.488074	9.976691	-0.059466	4.815549
292.083716	8000.524459	9.981696	-0.059455	4.815560
291.879738	8000.500778	9.986701	-0.059417	4.815554
292.081616	8000.524424	9.991706	-0.059455	4.815560
292.064096	8000.507033	9.996711	-0.059451	4.815555
291.847593	8000.446807	10.001715	-0.059411	4.815538
291.985873	8000.527114	10.006720	-0.059437	4.815561
291.970123	8000.475552	10.011725	-0.059434	4.815546
291.958531	8000.433679	10.016730	-0.059432	4.815534
291.974022	8000.535466	10.021735	-0.059435	4.815563
292.053723	8000.533578	10.026739	-0.059449	4.815562
292.028059	8000.522466	10.031744	-0.059445	4.815559
292.133556	8000.523142	10.036749	-0.059464	4.815559
292.352181	8000.529965	10.041754	-0.059505	4.815560
292.232295	8000.477749	10.046759	-0.059483	4.815545
292.100617	8000.448851	10.051763	-0.059458	4.815537
292.293326	8000.524715	10.056768	-0.059494	4.815559
292.264531	8000.532788	10.061773	-0.059489	4.815561
292.009106	8000.544593	10.066778	-0.059441	4.815566
292.009381	8000.532841	10.071783	-0.059441	4.815562
292.202779	8000.501840	10.076787	-0.059477	4.815552
292.277480	8000.536207	10.081792	-0.059491	4.815562
292.107225	8000.503465	10.086797	-0.059459	4.815553
292.262387	8000.528475	10.091802	-0.059488	4.815560
292.182462	8000.518602	10.096807	-0.059473	4.815557
291.971209	8000.500144	10.101811	-0.059434	4.815553
292.120462	8000.529332	10.106816	-0.059462	4.815561
292.041226	8000.494889	10.111821	-0.059447	4.815551
292.091765	8000.523513	10.116826	-0.059456	4.815559
292.017772	8000.540457	10.121831	-0.059443	4.815565
292.150970	8000.538385	10.126835	-0.059467	4.815563
292.392009	8000.526342	10.131840	-0.059512	4.815559
292.304566	8000.493900	10.136845	-0.059496	4.815550
292.324575	8000.510262	10.141850	-0.059500	4.815554
292.450224	8000.539060	10.146855	-0.059523	4.815562
292.161286	8000.530004	10.151859	-0.059469	4.815561
292.120758	8000.544296	10.156864	-0.059462	4.815565
292.177251	8000.511030	10.161869	-0.059472	4.815555
292.247180	8000.546387	10.166874	-0.059485	4.815565
292.141182	8000.500813	10.171879	-0.059465	4.815552
292.234976	8000.506640	10.176883	-0.059483	4.815554
292.383050	8000.505883	10.181888	-0.059511	4.815553
292.296939	8000.511939	10.186893	-0.059494	4.815555
292.266579	8000.547774	10.191898	-0.059489	4.815566
292.524904	8000.537086	10.196903	-0.059537	4.815561
292.311020	8000.529271	10.201907	-0.059497	4.815560
292.355347	8000.551379	10.206912	-0.059505	4.815566
292.415463	8000.523517	10.211917	-0.059517	4.815558
292.279702	8000.471038	10.216922	-0.059491	4.815543
292.326787	8000.543424	10.221927	-0.059500	4.815564
292.327190	8000.502817	10.226931	-0.059500	4.815552
292.502418	8000.543123	10.231936	-0.059533	4.815563
292.374868	8000.510018	10.236941	-0.059509	4.815554
292.331387	8000.537086	10.241946	-0.059501	4.815562
292.448301	8000.524058	10.246951	-0.059523	4.815558
292.385259	8000.511258	10.251955	-0.059511	4.815554
292.383925	8000.525129	10.256960	-0.059511	4.815558
292.275472	8000.477377	10.261965	-0.059490	4.815545
292.340853	8000.494490	10.266970	-0.059503	4.815550
292.390974	8000.500663	10.271975	-0.059512	4.815551
292.423415	8000.520437	10.276979	-0.059518	4.815557
292.690141	8000.556914	10.281984	-0.059568	4.815566
292.372990	8000.517464	10.286989	-0.059509	4.815556
292.330455	8000.521035	10.291994	-0.059501	4.815557
292.528172	8000.521100	10.296999	-0.059537	4.815557
292.516543	8000.497394	10.302003	-0.059535	4.815550
292.702160	8000.526116	10.307008	-0.059570	4.815557
292.494683	8000.491688	10.312013	-0.059531	4.815548
292.599297	8000.542582	10.317018	-0.059551	4.815562
292.591092	8000.528552	10.322023	-0.059549	4.815558
292.689616	8000.522700	10.327027	-0.059567	4.815556
292.756008	8000.468223	10.332032	-0.059580	4.815540
292.877642	8000.461685	10.337037	-0.059602	4.815537
292.849602	8000.500765	10.342042	-0.059597	4.815549
293.053221	8000.528716	10.347047	-0.059635	4.815556
292.986151	8000.498749	10.352051	-0.059623	4.815548
292.803760	8000.535275	10.357056	-0.059589	4.815559
292.902830	8000.478131	10.362061	-0.059607	4.815542
292.949844	8000.518454	10.367066	-0.059616	4.815554
292.948761	8000.543017	10.372071	-0.059616	4.815561
292.724956	8000.517937	10.377075	-0.059574	4.815555
292.920888	8000.541486	10.382080	-0.059610	4.815561
292.865757	8000.498891	10.387085	-0.059600	4.815548
292.856582	8000.522252	10.392090	-0.059599	4.815555
292.954568	8000.543111	10.397095	-0.059617	4.815561
292.963806	8000.522957	10.402099	-0.059618	4.815555
293.091573	8000.530415	10.407104	-0.059642	4.815557
292.972919	8000.508144	10.412109	-0.059620	4.815551
292.999028	8000.525676	10.417114	-0.059625	4.815556
293.027906	8000.552873	10.422119	-0.059630	4.815563
292.871681	8000.516086	10.427123	-0.059601	4.815553
293.054342	8000.543691	10.432128	-0.059635	4.815561
292.864477	8000.514898	10.437133	-0.059600	4.815553
292.759269	8000.475749	10.442138	-0.059580	4.815542
293.002464	8000.581308	10.447143	-0.059626	4.815572
292.845550	8000.561609	10.452147	-0.059596	4.815567
292.771127	8000.566790	10.457152	-0.059583	4.815569
292.961239	8000.523978	10.462157	-0.059618	4.815555
292.883163	8000.539786	10.467162	-0.059603	4.815560
292.882829	8000.530161	10.472167	-0.059603	4.815557
292.771595	8000.528320	10.477171	-0.059583	4.815557
292.888633	8000.554839	10.482176	-0.059604	4.815565
292.779843	8000.513493	10.487181	-0.059584	4.815553
292.834716	8000.524020	10.492186	-0.059594	4.815556
292.865054	8000.545897	10.497191	-0.059600	4.815562
292.936652	8000.523568	10.502195	-0.059613	4.815555
292.865462	8000.525596	10.507200	-0.059600	4.815556
292.943010	8000.517260	10.512205	-0.059614	4.815553
293.030285	8000.529392	10.517210	-0.059631	4.815557
293.139592	8000.549370	10.522215	-0.059651	4.815562
293.009852	8000.557910	10.527219	-0.059627	4.815565
293.169070	8000.494280	10.532224	-0.059657	4.815546
292.878288	8000.563213	10.537229	-0.059602	4.815567
292.784251	8000.573413	10.542234	-0.059585	4.815571
292.936370	8000.547073	10.547239	-0.059613	4.815562
292.885165	8000.513093	10.552243	-0.059604	4.815552
292.879370	8000.543991	10.557248	-0.059603	4.815562
293.094481	8000.529382	10.562253	-0.059643	4.815556
292.915877	8000.554214	10.567258	-0.059609	4.815564
292.886213	8000.555860	10.572263	-0.059604	4.815565
292.760788	8000.544165	10.577267	-0.059581	4.815562
293.271422	8000.557960	10.582272	-0.059676	4.815564
293.128528	8000.522462	10.587277	-0.059649	4.815554
292.930534	8000.555523	10.592282	-0.059612	4.815565
292.970935	8000.546572	10.597287	-0.059620	4.815562
292.908855	8000.535926	10.602291	-0.059608	4.815559
292.914055	8000.561662	10.607296	-0.059609	4.815567
292.903353	8000.527283	10.612301	-0.059607	4.815557
293.222571	8000.536842	10.617306	-0.059666	4.815558
293.208767	8000.557989	10.622311	-0.059664	4.815564
293.088260	8000.555993	10.627315	-0.059641	4.815564
293.201338	8000.456330	10.632320	-0.059662	4.815534
293.208388	8000.560119	10.637325	-0.059664	4.815565
293.104549	8000.563743	10.642330	-0.059644	4.815566
293.242904	8000.547864	10.647335	-0.059670	4.815561
292.964984	8000.549676	10.652339	-0.059618	4.815563
293.000797	8000.579125	10.657344	-0.059625	4.815571
292.772340	8000.550762	10.662349	-0.059583	4.815564
292.950506	8000.545160	10.667354	-0.059616	4.815562
293.005540	8000.547139	10.672359	-0.059626	4.815562
292.877313	8000.497990	10.677363	-0.059602	4.815548
292.937855	8000.535330	10.682368	-0.059613	4.815559
293.035721	8000.515574	10.687373	-0.059632	4.815552
293.037070	8000.518802	10.692378	-0.059632	4.815553
293.070529	8000.554626	10.697383	-0.059638	4.815564
292.959674	8000.527140	10.702387	-0.059617	4.815556
293.242425	8000.528613	10.707392	-0.059670	4.815555
293.196317	8000.512886	10.712397	-0.059661	4.815551
293.133903	8000.552467	10.717402	-0.059650	4.815563
293.086145	8000.551676	10.722407	-0.059641	4.815563
292.829208	8000.508947	10.727411	-0.059593	4.815552
292.871095	8000.554528	10.732416	-0.059601	4.815565
292.963257	8000.532540	10.737421	-0.059618	4.815558
293.104655	8000.515642	10.742426	-0.059644	4.815552
293.131752	8000.527846	10.747431	-0.059649	4.815556
293.109524	8000.508240	10.752435	-0.059645	4.815550
293.229230	8000.490983	10.757440	-0.059668	4.815544
293.105291	8000.481450	10.762445	-0.059644	4.815542
293.215428	8000.503579	10.767450	-0.059665	4.815548
293.316224	8000.499903	10.772455	-0.059684	4.815547
293.061440	8000.478585	10.777459	-0.059636	4.815542
293.339087	8000.546239	10.782464	-0.059688	4.815560
293.392526	8000.442381	10.787469	-0.059698	4.815529
293.191992	8000.565179	10.792474	-0.059661	4.815566
293.073322	8000.562145	10.797479	-0.059639	4.815566
293.150717	8000.530293	10.802483	-0.059653	4.815556
293.331866	8000.570699	10.807488	-0.059687	4.815567
293.171233	8000.558421	10.812493	-0.059657	4.815564
293.214127	8000.563405	10.817498	-0.059665	4.815566
293.261200	8000.564184	10.822503	-0.059673	4.815566
293.238542	8000.547777	10.827507	-0.059669	4.815561
293.268880	8000.569655	10.832512	-0.059675	4.815567
293.329688	8000.523634	10.837517	-0.059686	4.815553
293.382851	8000.551233	10.842522	-0.059696	4.815561
293.238580	8000.557395	10.847527	-0.059669	4.815564
293.313669	8000.562913	10.852531	-0.059683	4.815565
293.248770	8000.481679	10.857536	-0.059671	4.815542
293.238324	8000.554183	10.862541	-0.059669	4.815563
293.125215	8000.556586	10.867546	-0.059648	4.815564
293.391070	8000.535335	10.872551	-0.059698	4.815557
293.420932	8000.528347	10.877555	-0.059703	4.815554
293.443213	8000.554367	10.882560	-0.059707	4.815562
293.485470	8000.546516	10.887565	-0.059715	4.815559
293.454829	8000.542802	10.892570	-0.059709	4.815558
293.592582	8000.556839	10.897575	-0.059735	4.815562
293.277653	8000.488566	10.902579	-0.059676	4.815543
293.505245	8000.493402	10.907584	-0.059719	4.815544
293.371988	8000.556392	10.912589	-0.059694	4.815563
293.228498	8000.563635	10.917594	-0.059667	4.815566
293.368309	8000.580912	10.922599	-0.059693	4.815570
293.124793	8000.543748	10.927603	-0.059648	4.815560
293.194620	8000.488258	10.932608	-0.059661	4.815544
293.235875	8000.534898	10.937613	-0.059669	4.815557
293.246636	8000.536145	10.942618	-0.059671	4.815557
293.160563	8000.538995	10.947623	-0.059655	4.815559
293.198457	8000.512902	10.952627	-0.059662	4.815551
293.266121	8000.558911	10.957632	-0.059674	4.815564
293.167616	8000.550867	10.962637	-0.059656	4.815562
293.158741	8000.541101	10.967642	-0.059654	4.815559
293.279330	8000.533477	10.972647	-0.059677	4.815557
293.146293	8000.503486	10.977651	-0.059652	4.815548
293.295797	8000.543368	10.982656	-0.059680	4.815559
293.189698	8000.526649	10.987661	-0.059660	4.815555
293.260559	8000.550266	10.992666	-0.059673	4.815562
293.230902	8000.549774	10.997671	-0.059668	4.815562
293.187960	8000.512724	11.002675	-0.059660	4.815551
293.357923	8000.575390	11.007680	-0.059691	4.815568
293.151820	8000.537776	11.012685	-0.059653	4.815558
293.086273	8000.529209	11.017690	-0.059641	4.815556
293.393388	8000.553531	11.022695	-0.059698	4.815562
293.246362	8000.545753	11.027699	-0.059671	4.815560
293.156760	8000.479073	11.032704	-0.059654	4.815541
293.135119	8000.553530	11.037709	-0.059650	4.815563
293.211193	8000.562270	11.042714	-0.059664	4.815565
293.363634	8000.541280	11.047719	-0.059692	4.815558
293.245451	8000.511534	11.052723	-0.059670	4.815550
293.305986	8000.551012	11.057728	-0.059682	4.815562
293.208940	8000.530167	11.062733	-0.059664	4.815556
293.178584	8000.549971	11.067738	-0.059658	4.815562
293.353592	8000.548593	11.072743	-0.059690	4.815561
293.156930	8000.515411	11.077747	-0.059654	4.815552
293.138063	8000.538612	11.082752	-0.059650	4.815559
292.914371	8000.526359	11.087757	-0.059609	4.815556
293.149560	8000.553764	11.092762	-0.059652	4.815563
293.108710	8000.555225	11.097767	-0.059645	4.815564
293.137412	8000.512948	11.102771	-0.059650	4.815551
293.356371	8000.454583	11.107776	-0.059691	4.815533
293.381443	8000.513781	11.112781	-0.059696	4.815550
293.282234	8000.489693	11.117786	-0.059677	4.815544
293.489636	8000.566873	11.122791	-0.059716	4.815565
293.505655	8000.503010	11.127795	-0.059719	4.815547
293.366657	8000.544529	11.132800	-0.059693	4.815559
293.275475	8000.532331	11.137805	-0.059676	4.815556
293.320708	8000.527736	11.142810	-0.059684	4.815555
293.589190	8000.556762	11.147815	-0.059734	4.815562
293.163905	8000.475975	11.152819	-0.059655	4.815540
293.394548	8000.522544	11.157824	-0.059698	4.815553
293.340928	8000.541963	11.162829	-0.059688	4.815559
293.179027	8000.517907	11.167834	-0.059658	4.815552
293.380284	8000.539407	11.172839	-0.059695	4.815558
293.386277	8000.503167	11.177843	-0.059696	4.815547
293.431525	8000.516741	11.182848	-0.059705	4.815551
293.248108	8000.546837	11.187853	-0.059671	4.815561
293.575533	8000.561876	11.192858	-0.059732	4.815563
293.679977	8000.571087	11.197863	-0.059751	4.815566
293.583294	8000.498945	11.202867	-0.059733	4.815545
293.313158	8000.514780	11.207872	-0.059683	4.815551
293.556379	8000.530563	11.212877	-0.059728	4.815554
293.480335	8000.504721	11.217882	-0.059714	4.815547
293.594215	8000.565390	11.222887	-0.059735	4.815564
293.515971	8000.532030	11.227891	-0.059721	4.815555
293.348133	8000.549558	11.232896	-0.059689	4.815561
293.611200	8000.553913	11.237901	-0.059738	4.815561
293.640213	8000.527673	11.242906	-0.059744	4.815553
293.632797	8000.542513	11.247911	-0.059742	4.815557
293.304243	8000.497528	11.252915	-0.059681	4.815546
293.412946	8000.539941	11.257920	-0.059701	4.815558
293.410995	8000.535633	11.262925	-0.059701	4.815557
293.379235	8000.514800	11.267930	-0.059695	4.815551
293.383675	8000.540524	11.272935	-0.059696	4.815558
293.446984	8000.498820	11.277939	-0.059708	4.815546
293.391168	8000.562023	11.282944	-0.059697	4.815564
293.421240	8000.547558	11.287949	-0.059703	4.815560
293.429408	8000.503872	11.292954	-0.059704	4.815547
293.614535	8000.552894	11.297959	-0.059739	4.815561
293.605806	8000.508929	11.302963	-0.059737	4.815548
293.505272	8000.511539	11.307968	-0.059718	4.815549
293.501052	8000.503988	11.312973	-0.059718	4.815547
293.417475	8000.482297	11.317978	-0.059702	4.815541
293.444681	8000.538324	11.322983	-0.059707	4.815557
293.484318	8000.500503	11.327987	-0.059715	4.815546
293.431133	8000.530617	11.332992	-0.059705	4.815555
293.466082	8000.522645	11.337997	-0.059711	4.815552
293.705088	8000.492400	11.343002	-0.059756	4.815542
293.815712	8000.547671	11.348007	-0.059776	4.815558
293.462181	8000.497997	11.353011	-0.059710	4.815545
293.498742	8000.530666	11.358016	-0.059717	4.815555
293.578292	8000.511675	11.363021	-0.059732	4.815549
293.574552	8000.487030	11.368026	-0.059731	4.815542
293.609448	8000.553873	11.373031	-0.059738	4.815561
293.535392	8000.514170	11.378035	-0.059724	4.815550
293.643010	8000.537327	11.383040	-0.059744	4.815556
293.434261	8000.514633	11.388045	-0.059705	4.815550
293.548866	8000.442783	11.393050	-0.059726	4.815529
293.734439	8000.544184	11.398055	-0.059761	4.815557
293.403901	8000.511991	11.403059	-0.059699	4.815550
293.558337	8000.527373	11.408064	-0.059728	4.815553
293.644388	8000.529866	11.413069	-0.059744	4.815554
293.515239	8000.511696	11.418074	-0.059720	4.815549
293.474325	8000.546288	11.423079	-0.059713	4.815559
293.472273	8000.518465	11.428083	-0.059712	4.815551
293.588809	8000.553526	11.433088	-0.059734	4.815561
293.653574	8000.544979	11.438093	-0.059746	4.815558
293.596261	8000.519448	11.443098	-0.059735	4.815551
293.735656	8000.543131	11.448103	-0.059761	4.815557
293.471650	8000.506696	11.453107	-0.059712	4.815548
293.454231	8000.520302	11.458112	-0.059709	4.815552
293.683219	8000.493097	11.463117	-0.059751	4.815543
293.616442	8000.529399	11.468122	-0.059739	4.815554
293.730243	8000.545177	11.473127	-0.059760	4.815558
293.680149	8000.530453	11.478131	-0.059751	4.815554
293.714004	8000.542770	11.483136	-0.059757	4.815557
293.428682	8000.541252	11.488141	-0.059704	4.815558
293.318627	8000.509504	11.493146	-0.059684	4.815549
293.525535	8000.480864	11.498151	-0.059722	4.815540
293.580367	8000.390925	11.503155	-0.059732	4.815513
293.655067	8000.432775	11.508160	-0.059746	4.815525
293.591149	8000.512944	11.513165	-0.059734	4.815549
293.557425	8000.536968	11.518170	-0.059728	4.815556
293.664515	8000.501333	11.523175	-0.059748	4.815545
293.716121	8000.487223	11.528179	-0.059757	4.815541
293.617013	8000.501614	11.533184	-0.059739	4.815546
293.853089	8000.500178	11.538189	-0.059783	4.815544
293.725577	8000.508755	11.543194	-0.059759	4.815547
293.870110	8000.568863	11.548199	-0.059786	4.815564
293.869682	8000.541066	11.553203	-0.059786	4.815556
293.768253	8000.567175	11.558208	-0.059767	4.815564
293.915590	8000.552513	11.563213	-0.059795	4.815559
293.897681	8000.549010	11.568218	-0.059791	4.815558
293.905639	8000.550210	11.573223	-0.059793	4.815558
293.849378	8000.523627	11.578227	-0.059782	4.815551
293.832359	8000.527620	11.583232	-0.059779	4.815552
293.926464	8000.556967	11.588237	-0.059797	4.815560
293.886340	8000.553096	11.593242	-0.059789	4.815559
293.777348	8000.547015	11.598247	-0.059769	4.815558
293.705859	8000.514836	11.603251	-0.059756	4.815549
293.918174	8000.535452	11.608256	-0.059795	4.815554
293.923775	8000.559058	11.613261	-0.059796	4.815561
293.852312	8000.534360	11.618266	-0.059783	4.815554
293.871774	8000.504756	11.623271	-0.059786	4.815545
293.624740	8000.499597	11.628275	-0.059740	4.815545
293.873623	8000.544331	11.633280	-0.059787	4.815557
293.989280	8000.561209	11.638285	-0.059808	4.815561
293.669415	8000.518505	11.643290	-0.059749	4.815550
293.914234	8000.549278	11.648295	-0.059794	4.815558
294.054950	8000.524887	11.653299	-0.059820	4.815550
294.030185	8000.571504	11.658304	-0.059816	4.815564
293.922200	8000.450010	11.663309	-0.059796	4.815529
293.888726	8000.507170	11.668314	-0.059790	4.815546
293.823098	8000.544560	11.673319	-0.059777	4.815557
293.779680	8000.516052	11.678323	-0.059769	4.815549
293.897381	8000.540445	11.683328	-0.059791	4.815556
293.835794	8000.568283	11.688333	-0.059780	4.815564
293.647190	8000.538440	11.693338	-0.059745	4.815556
293.822123	8000.565918	11.698343	-0.059777	4.815563
293.855211	8000.527989	11.703347	-0.059783	4.815552
293.928269	8000.530267	11.708352	-0.059797	4.815552
293.870379	8000.542134	11.713357	-0.059786	4.815556
293.833081	8000.524415	11.718362	-0.059779	4.815551
293.932664	8000.582710	11.723367	-0.059798	4.815568
293.811210	8000.544359	11.728371	-0.059775	4.815557
293.912141	8000.554580	11.733376	-0.059794	4.815560
293.981946	8000.363351	11.738381	-0.059807	4.815503
293.831915	8000.577834	11.743386	-0.059779	4.815567
293.840282	8000.582247	11.748391	-0.059780	4.815568
293.880600	8000.566882	11.753395	-0.059788	4.815563
293.755969	8000.478245	11.758400	-0.059765	4.815538
293.762906	8000.546763	11.763405	-0.059766	4.815558
293.689935	8000.533798	11.768410	-0.059752	4.815555
293.896861	8000.507297	11.773415	-0.059791	4.815546
293.857246	8000.515191	11.778419	-0.059784	4.815548
293.883059	8000.542338	11.783424	-0.059788	4.815556
293.866056	8000.571982	11.788429	-0.059785	4.815565
293.659799	8000.548260	11.793434	-0.059747	4.815559
293.822742	8000.558439	11.798439	-0.059777	4.815561
293.630227	8000.530669	11.803443	-0.059741	4.815554
293.772683	8000.533027	11.808448	-0.059768	4.815554
293.886222	8000.533837	11.813453	-0.059789	4.815554
294.033076	8000.507411	11.818458	-0.059816	4.815545
293.983169	8000.558956	11.823463	-0.059807	4.815561
293.758885	8000.543485	11.828467	-0.059765	4.815557
293.794017	8000.580405	11.833472	-0.059772	4.815568
293.775509	8000.560860	11.838477	-0.059768	4.815562
293.757334	8000.535976	11.843482	-0.059765	4.815555
293.846184	8000.464768	11.848487	-0.059781	4.815534
293.793770	8000.521615	11.853491	-0.059772	4.815551
293.621603	8000.541209	11.858496	-0.059740	4.815557
293.750250	8000.559371	11.863501	-0.059764	4.815562
293.816032	8000.544428	11.868506	-0.059776	4.815557
293.948081	8000.571196	11.873511	-0.059800	4.815564
293.879908	8000.534796	11.878515	-0.059788	4.815554
293.747889	8000.543298	11.883520	-0.059763	4.815557
293.970683	8000.571569	11.888525	-0.059805	4.815564
293.888802	8000.559525	11.893530	-0.059789	4.815561
293.881644	8000.560475	11.898535	-0.059788	4.815562
293.812213	8000.546499	11.903539	-0.059775	4.815558
293.693360	8000.565907	11.908544	-0.059753	4.815564
293.734787	8000.570868	11.913549	-0.059761	4.815565
293.688521	8000.510249	11.918554	-0.059752	4.815548
293.789651	8000.576051	11.923559	-0.059771	4.815567
293.762879	8000.544612	11.928563	-0.059766	4.815557
293.873312	8000.572091	11.933568	-0.059786	4.815565
293.842948	8000.459364	11.938573	-0.059781	4.815532
293.695571	8000.507157	11.943578	-0.059753	4.815547
293.928283	8000.576206	11.948583	-0.059797	4.815566
293.758922	8000.534925	11.953587	-0.059765	4.815555
293.792104	8000.552575	11.958592	-0.059771	4.815560
293.711154	8000.566197	11.963597	-0.059756	4.815564
293.593705	8000.528982	11.968602	-0.059734	4.815554
293.806151	8000.557081	11.973607	-0.059774	4.815561
293.628872	8000.510325	11.978611	-0.059741	4.815548
293.801915	8000.493951	11.983616	-0.059773	4.815542
293.963057	8000.554334	11.988621	-0.059803	4.815559
293.944209	8000.542265	11.993626	-0.059800	4.815556
293.786532	8000.561030	11.998631	-0.059770	4.815562
293.787762	8000.531123	12.003635	-0.059770	4.815553
293.753363	8000.538035	12.008640	-0.059764	4.815556
293.709299	8000.552268	12.013645	-0.059756	4.815560
293.702407	8000.537190	12.018650	-0.059755	4.815556
293.793484	8000.578244	12.023655	-0.059772	4.815567
293.843080	8000.547000	12.028659	-0.059781	4.815558
293.718610	8000.562040	12.033664	-0.059758	4.815563
293.841108	8000.562999	12.038669	-0.059780	4.815562
293.620649	8000.525147	12.043674	-0.059739	4.815552
293.748327	8000.580700	12.048679	-0.059763	4.815568
293.745787	8000.564626	12.053683	-0.059763	4.815563
293.954147	8000.480433	12.058688	-0.059801	4.815538
293.876143	8000.573196	12.063693	-0.059787	4.815565
293.673337	8000.551668	12.068698	-0.059749	4.815560
293.837716	8000.555458	12.073703	-0.059780	4.815560
293.625082	8000.549800	12.078707	-0.059740	4.815560
293.861162	8000.539813	12.083712	-0.059784	4.815556
294.084447	8000.562749	12.088717	-0.059826	4.815561
293.804023	8000.523903	12.093722	-0.059773	4.815551
293.869678	8000.567742	12.098727	-0.059786	4.815564
293.676535	8000.539962	12.103731	-0.059750	4.815557
293.833598	8000.553250	12.108736	-0.059779	4.815560
293.756899	8000.542360	12.113741	-0.059765	4.815557
293.598597	8000.507675	12.118746	-0.059735	4.815547
293.889511	8000.542417	12.123751	-0.059789	4.815556
293.869941	8000.564538	12.128755	-0.059786	4.815563
293.759792	8000.477210	12.133760	-0.059765	4.815538
293.876535	8000.588160	12.138765	-0.059787	4.815570
293.807231	8000.560292	12.143770	-0.059774	4.815562
294.041923	8000.595173	12.148775	-0.059818	4.815571
293.899369	8000.559679	12.153779	-0.059791	4.815561
293.881999	8000.574354	12.158784	-0.059788	4.815566
293.784642	8000.574879	12.163789	-0.059770	4.815566
293.708898	8000.471020	12.168794	-0.059756	4.815536
293.858704	8000.573967	12.173799	-0.059784	4.815566
294.086375	8000.556361	12.178803	-0.059826	4.815559
293.934597	8000.566673	12.183808	-0.059798	4.815563
293.943741	8000.573237	12.188813	-0.059799	4.815565
293.659388	8000.534326	12.193818	-0.059746	4.815555
293.823307	8000.579792	12.198823	-0.059777	4.815567
293.806513	8000.467289	12.203827	-0.059774	4.815535
293.813173	8000.577486	12.208832	-0.059775	4.815567
293.970300	8000.587569	12.213837	-0.059804	4.815569
293.763028	8000.471912	12.218842	-0.059766	4.815536
293.942453	8000.593520	12.223847	-0.059799	4.815571
294.043312	8000.564194	12.228851	-0.059818	4.815562
293.823433	8000.555209	12.233856	-0.059777	4.815560
293.954135	8000.577680	12.238861	-0.059801	4.815566
294.024505	8000.457001	12.243866	-0.059814	4.815531
293.966466	8000.608879	12.248871	-0.059804	4.815575
293.861538	8000.564389	12.253875	-0.059784	4.815563
293.848524	8000.569517	12.258880	-0.059782	4.815564
293.817015	8000.492041	12.263885	-0.059776	4.815542
293.830508	8000.551048	12.268890	-0.059778	4.815559
294.038970	8000.587632	12.273895	-0.059817	4.815569
293.920891	8000.550406	12.278899	-0.059795	4.815558
293.791249	8000.553603	12.283904	-0.059771	4.815560
293.832567	8000.552149	12.288909	-0.059779	4.815559
293.822483	8000.528468	12.293914	-0.059777	4.815552
294.146090	8000.578716	12.298919	-0.059837	4.815566
294.013091	8000.538036	12.303923	-0.059812	4.815554
293.992648	8000.532353	12.308928	-0.059808	4.815553
294.082053	8000.594755	12.313933	-0.059825	4.815571
293.913201	8000.550275	12.318938	-0.059794	4.815558
294.036706	8000.480710	12.323943	-0.059816	4.815537
294.173916	8000.552454	12.328947	-0.059842	4.815558
294.025179	8000.576711	12.333952	-0.059814	4.815566
293.988719	8000.559006	12.338957	-0.059808	4.815561
294.058700	8000.541994	12.343962	-0.059821	4.815555
293.939058	8000.562458	12.348967	-0.059798	4.815562
293.802245	8000.525991	12.353971	-0.059773	4.815552
293.851819	8000.538568	12.358976	-0.059782	4.815555
294.113938	8000.573903	12.363981	-0.059831	4.815564
293.793396	8000.545081	12.368986	-0.059771	4.815557
293.818749	8000.583978	12.373991	-0.059776	4.815569
293.972919	8000.563016	12.378995	-0.059805	4.815562
293.891007	8000.537077	12.384000	-0.059789	4.815555
293.822550	8000.566938	12.389005	-0.059777	4.815564
293.819385	8000.534822	12.394010	-0.059776	4.815554
293.829159	8000.563841	12.399015	-0.059778	4.815563
293.827312	8000.552053	12.404019	-0.059777	4.815559
294.047633	8000.568526	12.409024	-0.059818	4.815563
294.099557	8000.560835	12.414029	-0.059828	4.815561
293.826981	8000.532808	12.419034	-0.059777	4.815554
293.943476	8000.557181	12.424039	-0.059799	4.815560
294.045017	8000.445568	12.429043	-0.059818	4.815527
293.988378	8000.571818	12.434048	-0.059807	4.815564
294.052090	8000.586767	12.439053	-0.059819	4.815568
294.162141	8000.536218	12.444058	-0.059840	4.815553
294.099095	8000.569375	12.449063	-0.059828	4.815563
294.090066	8000.543574	12.454067	-0.059826	4.815556
293.953707	8000.542384	12.459072	-0.059801	4.815556
294.064607	8000.563459	12.464077	-0.059822	4.815562
293.882930	8000.523042	12.469082	-0.059788	4.815551
293.919189	8000.537536	12.474087	-0.059794	4.815555
294.015760	8000.558373	12.479091	-0.059812	4.815560
293.982005	8000.561021	12.484096	-0.059806	4.815561
294.101711	8000.476429	12.489101	-0.059828	4.815536
294.034848	8000.507386	12.494106	-0.059816	4.815545
294.065403	8000.579501	12.499111	-0.059822	4.815566
293.898714	8000.560709	12.504115	-0.059791	4.815562
293.884720	8000.569027	12.509120	-0.059788	4.815564
294.137274	8000.485566	12.514125	-0.059835	4.815538
293.924352	8000.554719	12.519130	-0.059795	4.815560
293.987728	8000.568594	12.524135	-0.059807	4.815563
294.219332	8000.535020	12.529139	-0.059850	4.815552
294.013296	8000.552984	12.534144	-0.059812	4.815559
294.011168	8000.561499	12.539149	-0.059812	4.815561
294.030099	8000.541505	12.544154	-0.059815	4.815555
294.203509	8000.555064	12.549159	-0.059847	4.815558
293.993978	8000.561213	12.554163	-0.059808	4.815561
294.029660	8000.568216	12.559168	-0.059815	4.815563
294.181004	8000.591030	12.564173	-0.059843	4.815569
294.122284	8000.525928	12.569178	-0.059832	4.815550
294.107294	8000.571638	12.574183	-0.059829	4.815564
294.153997	8000.551035	12.579187	-0.059838	4.815557
294.119794	8000.562225	12.584192	-0.059832	4.815561
294.047885	8000.492630	12.589197	-0.059818	4.815541
293.875269	8000.558176	12.594202	-0.059786	4.815561
294.010072	8000.598884	12.599207	-0.059811	4.815572
293.871478	8000.554906	12.604211	-0.059785	4.815560
293.857251	8000.554670	12.609216	-0.059783	4.815560
294.200301	8000.484464	12.614221	-0.059847	4.815538
294.159267	8000.545775	12.619226	-0.059839	4.815556
293.833631	8000.557484	12.624231	-0.059778	4.815561
293.994661	8000.545186	12.629235	-0.059808	4.815557
294.048790	8000.566390	12.634240	-0.059818	4.815562
294.115957	8000.574983	12.639245	-0.059831	4.815565
293.873159	8000.534623	12.644250	-0.059786	4.815554
294.031741	8000.473120	12.649255	-0.059815	4.815535
294.163232	8000.449645	12.654259	-0.059840	4.815528
294.156726	8000.451675	12.659264	-0.059838	4.815528
294.425433	8000.551248	12.664269	-0.059889	4.815556
294.319199	8000.528112	12.669274	-0.059869	4.815550
294.393091	8000.516509	12.674279	-0.059883	4.815546
294.348203	8000.571344	12.679283	-0.059874	4.815562
294.386478	8000.578391	12.684288	-0.059881	4.815564
294.319843	8000.491781	12.689293	-0.059869	4.815539
294.240020	8000.565276	12.694298	-0.059854	4.815561
294.294257	8000.592894	12.699303	-0.059864	4.815569
294.277051	8000.560544	12.704307	-0.059861	4.815560
294.260025	8000.544230	12.709312	-0.059858	4.815555
294.350260	8000.578857	12.714317	-0.059875	4.815565
294.402648	8000.558348	12.719322	-0.059884	4.815558
294.292983	8000.595009	12.724327	-0.059864	4.815570
294.320532	8000.470413	12.729331	-0.059869	4.815533
294.490686	8000.575837	12.734336	-0.059901	4.815563
294.523097	8000.596681	12.739341	-0.059907	4.815569
294.346110	8000.563823	12.744346	-0.059874	4.815560
294.266462	8000.594568	12.749351	-0.059859	4.815570
294.322293	8000.488610	12.754355	-0.059869	4.815538
294.342575	8000.569107	12.759360	-0.059873	4.815562
294.480417	8000.572458	12.764365	-0.059899	4.815562
294.251463	8000.551565	12.769370	-0.059856	4.815557
294.217611	8000.567036	12.774375	-0.059850	4.815562
294.309246	8000.561072	12.779379	-0.059867	4.815560
294.372442	8000.551430	12.784384	-0.059879	4.815557
294.661788	8000.577598	12.789389	-0.059932	4.815563
294.513336	8000.543074	12.794394	-0.059905	4.815553
294.579717	8000.544173	12.799399	-0.059917	4.815553
294.633939	8000.568585	12.804403	-0.059927	4.815560
294.348567	8000.551032	12.809408	-0.059874	4.815557
294.436695	8000.573868	12.814413	-0.059891	4.815563
294.532394	8000.566902	12.819418	-0.059908	4.815560
294.524896	8000.582809	12.824423	-0.059907	4.815565
294.271126	8000.473862	12.829427	-0.059860	4.815534
294.306063	8000.581322	12.834432	-0.059866	4.815566
294.579597	8000.589058	12.839437	-0.059917	4.815567
294.415476	8000.547862	12.844442	-0.059887	4.815555
294.473096	8000.574468	12.849447	-0.059897	4.815563
294.608573	8000.452728	12.854451	-0.059922	4.815527
294.420677	8000.572530	12.859456	-0.059888	4.815562
294.414376	8000.605559	12.864461	-0.059886	4.815572
294.421751	8000.549033	12.869466	-0.059888	4.815556
294.414687	8000.478374	12.874471	-0.059886	4.815535
294.431051	8000.578044	12.879475	-0.059889	4.815564
294.241919	8000.549260	12.884480	-0.059854	4.815557
294.441458	8000.589973	12.889485	-0.059891	4.815567
294.338758	8000.553000	12.894490	-0.059872	4.815557
294.508526	8000.499164	12.899495	-0.059904	4.815541
294.595090	8000.587172	12.904499	-0.059920	4.815566
294.375147	8000.581391	12.909504	-0.059879	4.815565
294.445364	8000.564384	12.914509	-0.059892	4.815560
294.542500	8000.476211	12.919514	-0.059910	4.815534
294.413902	8000.577757	12.924519	-0.059886	4.815564
294.340227	8000.571192	12.929523	-0.059872	4.815562
294.307221	8000.547131	12.934528	-0.059866	4.815556
294.524480	8000.562486	12.939533	-0.059907	4.815559
294.282016	8000.561676	12.944538	-0.059862	4.815560
294.295719	8000.583279	12.949543	-0.059864	4.815566
294.456019	8000.577383	12.954547	-0.059894	4.815564
294.288286	8000.557503	12.959552	-0.059863	4.815559
294.340948	8000.578683	12.964557	-0.059873	4.815565
294.283953	8000.529642	12.969562	-0.059862	4.815551
294.286997	8000.430292	12.974567	-0.059862	4.815522
294.268212	8000.527243	12.979571	-0.059859	4.815550
294.463785	8000.541169	12.984576	-0.059895	4.815553
294.521334	8000.595563	12.989581	-0.059906	4.815569
294.276156	8000.531648	12.994586	-0.059860	4.815551
294.252053	8000.576139	12.999591	-0.059856	4.815564
294.460619	8000.575317	13.004595	-0.059895	4.815563
294.357839	8000.508417	13.009600	-0.059876	4.815544
294.515266	8000.590116	13.014605	-0.059905	4.815567
294.457066	8000.481201	13.019610	-0.059894	4.815536
294.335948	8000.563632	13.024615	-0.059872	4.815560
294.300128	8000.557694	13.029619	-0.059865	4.815559
294.326993	8000.546381	13.034624	-0.059870	4.815555
294.600340	8000.570147	13.039629	-0.059921	4.815561
294.291863	8000.529767	13.044634	-0.059863	4.815551
294.285286	8000.529657	13.049639	-0.059862	4.815551
294.526164	8000.556091	13.054643	-0.059907	4.815557
294.437980	8000.540736	13.059648	-0.059891	4.815553
294.344665	8000.584080	13.064653	-0.059873	4.815566
294.465988	8000.561506	13.069658	-0.059896	4.815559
294.345668	8000.498591	13.074663	-0.059873	4.815541
294.389378	8000.584820	13.079667	-0.059882	4.815566
294.277826	8000.561595	13.084672	-0.059861	4.815560
294.400930	8000.591423	13.089677	-0.059884	4.815568
294.216686	8000.543481	13.094682	-0.059849	4.815555
294.081064	8000.571162	13.099687	-0.059824	4.815564
294.429738	8000.465778	13.104691	-0.059889	4.815531
294.286248	8000.555320	13.109696	-0.059862	4.815558
294.330777	8000.579571	13.114701	-0.059871	4.815565
294.382750	8000.543023	13.119706	-0.059880	4.815554
294.284727	8000.584152	13.124711	-0.059862	4.815567
294.176211	8000.584492	13.129715	-0.059842	4.815567
294.212391	8000.561577	13.134720	-0.059848	4.815560
294.301346	8000.580150	13.139725	-0.059865	4.815565
294.240369	8000.538525	13.144730	-0.059854	4.815553
294.215536	8000.454746	13.149735	-0.059849	4.815529
294.328667	8000.557088	13.154739	-0.059870	4.815558
294.271698	8000.545456	13.159744	-0.059860	4.815555
294.481705	8000.559621	13.164749	-0.059899	4.815558
294.514622	8000.525964	13.169754	-0.059905	4.815548
294.574801	8000.584676	13.174759	-0.059916	4.815565
294.619693	8000.557630	13.179763	-0.059924	4.815557
294.492933	8000.545911	13.184768	-0.059901	4.815554
294.525123	8000.562476	13.189773	-0.059907	4.815559
294.453035	8000.544181	13.194778	-0.059893	4.815554
294.316447	8000.555813	13.199783	-0.059868	4.815558
294.455632	8000.557049	13.204787	-0.059894	4.815558
294.414808	8000.506138	13.209792	-0.059886	4.815543
294.510272	8000.573985	13.214797	-0.059904	4.815562
294.584990	8000.460858	13.219802	-0.059918	4.815529
294.516132	8000.575150	13.224807	-0.059905	4.815563
294.462371	8000.567846	13.229811	-0.059895	4.815561
294.353869	8000.556430	13.234816	-0.059875	4.815558
294.650558	8000.580582	13.239821	-0.059930	4.815564
294.786682	8000.550771	13.244826	-0.059955	4.815554
294.529154	8000.572157	13.249831	-0.059907	4.815562
294.585479	8000.572021	13.254835	-0.059918	4.815562
294.493467	8000.497817	13.259840	-0.059901	4.815540
294.469555	8000.540173	13.264845	-0.059896	4.815553
294.370735	8000.539605	13.269850	-0.059878	4.815553
294.449574	8000.566562	13.274855	-0.059893	4.815561
294.575418	8000.577196	13.279859	-0.059916	4.815563
294.370067	8000.496840	13.284864	-0.059878	4.815541
294.606009	8000.533881	13.289869	-0.059922	4.815550
294.671323	8000.555270	13.294874	-0.059934	4.815556
294.502041	8000.581324	13.299879	-0.059902	4.815565
294.449137	8000.553727	13.304883	-0.059892	4.815557
294.535244	8000.555152	13.309888	-0.059908	4.815557
294.602863	8000.554134	13.314893	-0.059921	4.815556
294.395342	8000.532527	13.319898	-0.059882	4.815551
294.562936	8000.523545	13.324903	-0.059914	4.815547
294.484478	8000.573549	13.329907	-0.059899	4.815562
294.218803	8000.527465	13.334912	-0.059849	4.815550
294.466193	8000.542249	13.339917	-0.059896	4.815553
294.606105	8000.523189	13.344922	-0.059922	4.815547
294.423522	8000.524441	13.349927	-0.059888	4.815548
294.412421	8000.559527	13.354931	-0.059886	4.815559
294.349606	8000.503977	13.359936	-0.059874	4.815543
294.380850	8000.536559	13.364941	-0.059880	4.815552
294.347799	8000.547768	13.369946	-0.059873	4.815556
294.545426	8000.551040	13.374951	-0.059910	4.815556
294.503793	8000.566383	13.379955	-0.059903	4.815560
294.283065	8000.530662	13.384960	-0.059861	4.815551
294.505912	8000.536490	13.389965	-0.059903	4.815552
294.483826	8000.528642	13.394970	-0.059899	4.815549
294.366189	8000.574790	13.399975	-0.059877	4.815563
294.463041	8000.575325	13.404979	-0.059895	4.815563
294.587141	8000.530352	13.409984	-0.059918	4.815549
294.648907	8000.554889	13.414989	-0.059930	4.815556
294.421719	8000.553263	13.419994	-0.059887	4.815557
294.520292	8000.563446	13.424999	-0.059906	4.815559
294.490149	8000.552258	13.430003	-0.059900	4.815556
294.483366	8000.536113	13.435008	-0.059899	4.815552
294.435914	8000.559910	13.440013	-0.059890	4.815559
294.566773	8000.500085	13.445018	-0.059914	4.815541
294.502424	8000.411376	13.450023	-0.059902	4.815515
294.669869	8000.572334	13.455027	-0.059933	4.815561
294.710176	8000.545211	13.460032	-0.059941	4.815553
294.647830	8000.573037	13.465037	-0.059929	4.815562
294.573927	8000.541885	13.470042	-0.059915	4.815553
294.770835	8000.570798	13.475047	-0.059952	4.815560
294.888614	8000.587712	13.480051	-0.059974	4.815565
294.642726	8000.539817	13.485056	-0.059928	4.815552
294.559800	8000.556613	13.490061	-0.059913	4.815557
294.666763	8000.564797	13.495066	-0.059933	4.815559
294.609821	8000.560647	13.500071	-0.059922	4.815558
294.608206	8000.572377	13.505075	-0.059922	4.815562
294.497923	8000.538486	13.510080	-0.059901	4.815552
294.673713	8000.553154	13.515085	-0.059934	4.815556
294.718564	8000.515418	13.520090	-0.059942	4.815544
294.805352	8000.546783	13.525095	-0.059959	4.815553
294.912937	8000.579560	13.530099	-0.059979	4.815562
294.643748	8000.534486	13.535104	-0.059928	4.815550
294.565571	8000.556705	13.540109	-0.059914	4.815557
294.667561	8000.548774	13.545114	-0.059933	4.815554
294.637953	8000.556834	13.550119	-0.059927	4.815557
294.691426	8000.465800	13.555123	-0.059937	4.815530
294.772758	8000.544102	13.560128	-0.059952	4.815552
294.776742	8000.580508	13.565133	-0.059953	4.815563
294.430149	8000.554459	13.570138	-0.059889	4.815557
294.437201	8000.529993	13.575143	-0.059890	4.815550
294.582337	8000.560186	13.580147	-0.059917	4.815558
294.539781	8000.532760	13.585152	-0.059909	4.815550
294.517107	8000.565517	13.590157	-0.059905	4.815560
294.674605	8000.559575	13.595162	-0.059934	4.815557
294.549502	8000.515819	13.600167	-0.059911	4.815545
294.648539	8000.573037	13.605171	-0.059929	4.815562
294.808716	8000.550038	13.610176	-0.059959	4.815554
294.522974	8000.585920	13.615181	-0.059906	4.815566
294.496510	8000.556623	13.620186	-0.059901	4.815557
294.652412	8000.564549	13.625191	-0.059930	4.815559
294.860825	8000.585102	13.630195	-0.059969	4.815564
294.762080	8000.555676	13.635200	-0.059950	4.815556
294.673009	8000.486865	13.640205	-0.059934	4.815536
294.812528	8000.594989	13.645210	-0.059960	4.815567
294.858602	8000.484594	13.650215	-0.059968	4.815535
294.898255	8000.592133	13.655219	-0.059976	4.815566
294.847068	8000.567770	13.660224	-0.059966	4.815559
294.819017	8000.580131	13.665229	-0.059961	4.815563
294.640136	8000.541897	13.670234	-0.059928	4.815552
294.484420	8000.546799	13.675239	-0.059899	4.815555
294.688305	8000.558726	13.680243	-0.059937	4.815557
294.592306	8000.507970	13.685248	-0.059919	4.815543
294.792426	8000.532660	13.690253	-0.059956	4.815549
294.670152	8000.533841	13.695258	-0.059933	4.815550
294.665259	8000.524140	13.700263	-0.059932	4.815547
294.819994	8000.566250	13.705267	-0.059961	4.815559
294.636701	8000.531148	13.710272	-0.059927	4.815549
294.760240	8000.556708	13.715277	-0.059950	4.815556
294.729419	8000.559404	13.720282	-0.059944	4.815557
294.793903	8000.563678	13.725287	-0.059956	4.815558
295.019736	8000.479774	13.730291	-0.059998	4.815532
294.794299	8000.561546	13.735296	-0.059956	4.815557
294.944738	8000.566175	13.740301	-0.059984	4.815558
294.959631	8000.547183	13.745306	-0.059987	4.815552
294.922340	8000.504880	13.750311	-0.059980	4.815540
294.805598	8000.557456	13.755315	-0.059958	4.815556
294.797958	8000.539159	13.760320	-0.059957	4.815551
294.948730	8000.575859	13.765325	-0.059985	4.815561
294.936228	8000.576720	13.770330	-0.059983	4.815561
294.727685	8000.562577	13.775335	-0.059944	4.815558
294.830154	8000.582444	13.780339	-0.059963	4.815563
294.925127	8000.543401	13.785344	-0.059981	4.815552
294.924193	8000.592552	13.790349	-0.059980	4.815566
294.853123	8000.455633	13.795354	-0.059967	4.815526
295.030171	8000.582549	13.800359	-0.060000	4.815562
294.934940	8000.597004	13.805363	-0.059982	4.815567
294.819597	8000.541651	13.810368	-0.059961	4.815552
294.770016	8000.582514	13.815373	-0.059952	4.815564
294.702464	8000.563225	13.820378	-0.059939	4.815558
294.614875	8000.550016	13.825383	-0.059923	4.815555
294.709615	8000.494938	13.830387	-0.059940	4.815538
294.821066	8000.545949	13.835392	-0.059961	4.815553
294.615891	8000.550032	13.840397	-0.059923	4.815555
294.709752	8000.566550	13.845402	-0.059940	4.815559
294.954092	8000.547082	13.850407	-0.059986	4.815552
295.020345	8000.592002	13.855411	-0.059998	4.815565
294.717726	8000.554924	13.860416	-0.059942	4.815556
294.793564	8000.586107	13.865421	-0.059956	4.815565
294.906657	8000.467202	13.870426	-0.059977	4.815529
294.692406	8000.541677	13.875431	-0.059937	4.815552
294.919228	8000.579636	13.880435	-0.059979	4.815562
294.707952	8000.552622	13.885440	-0.059940	4.815555
294.711570	8000.581540	13.890445	-0.059941	4.815564
294.683825	8000.558635	13.895450	-0.059936	4.815557
294.828973	8000.540731	13.900455	-0.059963	4.815551
295.032359	8000.560132	13.905459	-0.060000	4.815556
294.784715	8000.534653	13.910464	-0.059954	4.815550
294.704517	8000.565389	13.915469	-0.059939	4.815559
294.817753	8000.555507	13.920474	-0.059960	4.815556
294.724375	8000.527239	13.925479	-0.059943	4.815548
294.816245	8000.573651	13.930483	-0.059960	4.815561
294.832777	8000.557892	13.935488	-0.059963	4.815556
294.689771	8000.539491	13.940493	-0.059937	4.815552
294.679215	8000.538247	13.945498	-0.059935	4.815551
294.690362	8000.519192	13.950503	-0.059937	4.815546
295.054571	8000.481402	13.955507	-0.060005	4.815533
294.630098	8000.565221	13.960512	-0.059926	4.815559
294.885452	8000.587621	13.965517	-0.059973	4.815565
295.074247	8000.569371	13.970522	-0.060008	4.815558
294.890504	8000.490440	13.975527	-0.059974	4.815536
294.691594	8000.605785	13.980531	-0.059937	4.815571
294.985939	8000.588215	13.985536	-0.059992	4.815564
294.877340	8000.582140	13.990541	-0.059972	4.815563
294.864566	8000.481458	13.995546	-0.059969	4.815534
294.754242	8000.593995	14.000551	-0.059949	4.815567
294.866804	8000.581964	14.005555	-0.059970	4.815563
294.612618	8000.554239	14.010560	-0.059922	4.815556
294.729319	8000.587168	14.015565	-0.059944	4.815565
294.809599	8000.569258	14.020570	-0.059959	4.815560
294.808104	8000.561751	14.025575	-0.059959	4.815557
294.768691	8000.579268	14.030579	-0.059951	4.815563
294.758510	8000.531002	14.035584	-0.059949	4.815549
294.996795	8000.572358	14.040589	-0.059994	4.815560
294.870790	8000.554237	14.045594	-0.059970	4.815555
294.793324	8000.530509	14.050599	-0.059956	4.815548
294.928625	8000.488927	14.055603	-0.059981	4.815536
294.893871	8000.567445	14.060608	-0.059975	4.815559
294.866449	8000.564852	14.065613	-0.059969	4.815558
294.889272	8000.585538	14.070618	-0.059974	4.815564
294.662518	8000.549717	14.075623	-0.059931	4.815555
294.782093	8000.577349	14.080627	-0.059954	4.815562
294.691327	8000.528816	14.085632	-0.059937	4.815548
294.741900	8000.577751	14.090637	-0.059946	4.815562
294.919516	8000.549696	14.095642	-0.059979	4.815553
294.785046	8000.539987	14.100647	-0.059954	4.815551
294.878290	8000.568252	14.105651	-0.059972	4.815559
294.767102	8000.501211	14.110656	-0.059951	4.815540
294.949639	8000.579052	14.115661	-0.059985	4.815562
295.021076	8000.527862	14.120666	-0.059998	4.815547
294.911452	8000.545285	14.125671	-0.059978	4.815552
294.684032	8000.572514	14.130675	-0.059935	4.815561
294.794494	8000.531590	14.135680	-0.059956	4.815549
294.827055	8000.539611	14.140685	-0.059962	4.815551
294.798334	8000.556236	14.145690	-0.059957	4.815556
294.732047	8000.557275	14.150695	-0.059944	4.815557
294.898444	8000.576063	14.155699	-0.059975	4.815561
294.949941	8000.555539	14.160704	-0.059985	4.815555
294.854310	8000.579607	14.165709	-0.059967	4.815562
294.837007	8000.560081	14.170714	-0.059964	4.815557
294.743269	8000.544633	14.175719	-0.059946	4.815553
294.821113	8000.556610	14.180723	-0.059961	4.815556
294.824307	8000.466881	14.185728	-0.059961	4.815530
294.795893	8000.508094	14.190733	-0.059956	4.815542
294.743561	8000.548912	14.195738	-0.059946	4.815554
295.002998	8000.557484	14.200743	-0.059995	4.815555
295.131903	8000.569238	14.205747	-0.060019	4.815558
294.839245	8000.545151	14.210752	-0.059964	4.815552
294.990025	8000.572231	14.215757	-0.059992	4.815560
295.070312	8000.544702	14.220762	-0.060007	4.815551
295.134762	8000.521186	14.225767	-0.060019	4.815544
294.992216	8000.573335	14.230771	-0.059993	4.815560
294.909211	8000.545239	14.235776	-0.059977	4.815552
294.979728	8000.569921	14.240781	-0.059990	4.815559
295.143097	8000.585453	14.245786	-0.060021	4.815563
295.001254	8000.548900	14.250791	-0.059994	4.815553
295.121293	8000.496378	14.255795	-0.060017	4.815537
295.066654	7999.414920	14.260800	-0.060006	4.815221
295.043398	7996.186127	14.265805	-0.059999	4.814278
294.962292	7990.652782	14.270810	-0.059981	4.812662
294.904579	7983.885202	14.275815	-0.059965	4.810683
294.885242	7976.662110	14.280819	-0.059957	4.808571
294.898438	7968.998935	14.285824	-0.059955	4.806329
294.865050	7961.209593	14.290829	-0.059943	4.804049
294.731344	7953.369134	14.295834	-0.059913	4.801753
294.635487	7945.350904	14.300839	-0.059890	4.799404
294.744813	7937.468560	14.305843	-0.059905	4.797093
294.655998	7929.422090	14.310848	-0.059884	4.794733
294.587868	7921.356527	14.315853	-0.059866	4.792367
294.682915	7913.384518	14.320858	-0.059878	4.790026
294.668810	7905.370192	14.325863	-0.059870	4.787672
294.659494	7897.394939	14.330867	-0.059863	4.785328
294.593610	7889.368680	14.335872	-0.059846	4.782969
294.664732	7881.383304	14.340877	-0.059854	4.780619
294.637620	7873.402631	14.345882	-0.059844	4.778271
294.373106	7865.382466	14.350887	-0.059789	4.775910
294.375600	7857.356099	14.355891	-0.059784	4.773546
294.401680	7849.410266	14.360896	-0.059784	4.771203
294.231657	7841.369524	14.365901	-0.059747	4.768833
294.145961	7833.397383	14.370906	-0.059726	4.766481
294.168319	7825.339616	14.375911	-0.059725	4.764102
294.104999	7817.382064	14.380915	-0.059708	4.761753
293.877823	7809.345181	14.385920	-0.059660	4.759379
293.952864	7801.400413	14.390925	-0.059669	4.757030
294.041252	7793.324632	14.395930	-0.059680	4.754641
293.890473	7785.279701	14.400935	-0.059647	4.752260
294.167797	7777.265782	14.405939	-0.059694	4.749887
294.107622	7769.322667	14.410944	-0.059677	4.747534
293.931214	7761.302230	14.415949	-0.059639	4.745158
294.045136	7753.416325	14.420954	-0.059655	4.742819
294.016364	7745.281343	14.425959	-0.059644	4.740406
293.905171	7737.341066	14.430963	-0.059619	4.738049
293.996583	7729.306968	14.435968	-0.059630	4.735663
293.939317	7721.296445	14.440973	-0.059614	4.733283
293.852089	7713.305444	14.445978	-0.059593	4.730908
293.589213	7705.266471	14.450983	-0.059539	4.728518
293.781896	7697.295660	14.455987	-0.059569	4.726145
293.676713	7689.292550	14.460992	-0.059545	4.723763
293.576046	7681.323953	14.465997	-0.059521	4.721389
293.566393	7673.347629	14.471002	-0.059514	4.719012
293.735091	7665.343345	14.476007	-0.059540	4.716625
293.626946	7657.303108	14.481011	-0.059515	4.714227
293.469743	7649.282303	14.486016	-0.059480	4.711833
293.390697	7641.251626	14.491021	-0.059460	4.709435
293.641097	7633.295506	14.496026	-0.059502	4.707058
293.382418	7625.262248	14.501031	-0.059448	4.704657
293.366813	7617.317412	14.506035	-0.059440	4.702281
293.638180	7609.283723	14.511040	-0.059485	4.699876
293.230782	7601.337983	14.516045	-0.059404	4.697498
293.213723	7593.321941	14.521050	-0.059396	4.695097
293.160937	7585.266041	14.526055	-0.059381	4.692683
293.173883	7577.255327	14.531059	-0.059378	4.690281
293.146296	7569.275522	14.536064	-0.059368	4.687887
293.194539	7561.239951	14.541069	-0.059371	4.685475
293.497184	7553.341959	14.546074	-0.059423	4.683102
293.089662	7545.281876	14.551079	-0.059341	4.680681
293.115621	7537.273091	14.556083	-0.059341	4.678273
293.202626	7529.270818	14.561088	-0.059352	4.675866
293.111648	7521.183599	14.566093	-0.059330	4.673433
292.903382	7513.163312	14.571098	-0.059286	4.671018
292.924543	7505.178355	14.576103	-0.059285	4.668613
293.171238	7497.232675	14.581107	-0.059325	4.666217
292.793080	7489.263533	14.586112	-0.059250	4.663815
292.608953	7481.210462	14.591117	-0.059210	4.661385
292.905845	7473.242073	14.596122	-0.059260	4.658979
292.900824	7465.244571	14.601127	-0.059254	4.656564
292.775276	7457.236359	14.606131	-0.059225	4.654144
292.724291	7449.190284	14.611136	-0.059211	4.651711
292.794748	7441.177702	14.616141	-0.059219	4.649287
292.660609	7433.251201	14.621146	-0.059188	4.646888
292.540106	7425.186653	14.626151	-0.059161	4.644446
292.625055	7417.270094	14.631155	-0.059171	4.642048
292.346074	7409.229112	14.636160	-0.059114	4.639610
292.477135	7401.251970	14.641165	-0.059133	4.637191
292.446127	7393.201509	14.646170	-0.059122	4.634748
292.519638	7385.169878	14.651175	-0.059131	4.632309
292.373446	7377.161656	14.656179	-0.059098	4.629877
292.484702	7369.221704	14.661184	-0.059114	4.627463
292.248225	7361.155135	14.666189	-0.059065	4.625010
292.286951	7353.203978	14.671194	-0.059067	4.622591
292.192559	7345.149231	14.676199	-0.059044	4.620139
292.247775	7337.232095	14.681203	-0.059049	4.617728
292.247669	7329.177725	14.686208	-0.059044	4.615273
292.261140	7321.189069	14.691213	-0.059041	4.612837
292.177911	7313.118703	14.696218	-0.059020	4.610375
291.872039	7305.163186	14.701223	-0.058958	4.607947
291.823520	7297.160768	14.706227	-0.058944	4.605503
291.860653	7289.193213	14.711232	-0.058946	4.603069
292.028141	7281.160332	14.716237	-0.058972	4.600613
291.856753	7273.217751	14.721242	-0.058934	4.598183
291.618018	7265.122472	14.726247	-0.058885	4.595706
291.911598	7257.112438	14.731251	-0.058934	4.593253
291.930652	7249.108042	14.736256	-0.058932	4.590801
291.740055	7241.092017	14.741261	-0.058892	4.588343
291.951202	7233.108051	14.746266	-0.058926	4.585895
291.814251	7225.116841	14.751271	-0.058895	4.583442
291.772747	7217.101276	14.756275	-0.058882	4.580981
291.668671	7209.141006	14.761280	-0.058858	4.578536
291.644327	7201.155367	14.766285	-0.058848	4.576081
291.648291	7193.143498	14.771290	-0.058843	4.573618
291.376563	7185.081041	14.776295	-0.058788	4.571136
291.436499	7177.125364	14.781299	-0.058793	4.568687
291.493824	7169.107073	14.786304	-0.058799	4.566217
291.445524	7161.147177	14.791309	-0.058785	4.563764
291.591446	7153.138187	14.796314	-0.058807	4.561295
291.650746	7145.124742	14.801319	-0.058813	4.558822
291.570881	7137.133420	14.806323	-0.058792	4.556355
291.457222	7129.104178	14.811328	-0.058766	4.553875
291.569704	7121.061124	14.816333	-0.058782	4.551390
291.499182	7113.110139	14.821338	-0.058763	4.548931
291.467682	7105.080561	14.826343	-0.058752	4.546447
291.360268	7097.138478	14.831347	-0.058727	4.543988
291.377729	7089.147651	14.836352	-0.058725	4.541514
291.046513	7081.112809	14.841357	-0.058658	4.539023
291.212250	7073.161124	14.846362	-0.058684	4.536558
291.004297	7065.096254	14.851367	-0.058640	4.534056
291.041303	7057.082653	14.856371	-0.058642	4.531569
290.937043	7049.092450	14.861376	-0.058617	4.529087
291.069454	7041.089027	14.866381	-0.058636	4.526600
291.081365	7033.111866	14.871386	-0.058633	4.524120
290.789479	7025.105107	14.876391	-0.058574	4.521629
290.981759	7017.092354	14.881395	-0.058604	4.519135
291.041762	7009.140064	14.886400	-0.058610	4.516659
291.024012	7001.044466	14.891405	-0.058602	4.514136
290.993815	6993.009569	14.896410	-0.058591	4.511631
290.695450	6985.027331	14.901415	-0.058530	4.509140
290.760186	6977.047646	14.906419	-0.058537	4.506650
290.694067	6969.066458	14.911424	-0.058520	4.504157
290.719405	6961.077948	14.916429	-0.058519	4.501661
290.698945	6953.075302	14.921434	-0.058510	4.499159
290.658529	6945.063335	14.926439	-0.058497	4.496653
290.712229	6937.048013	14.931443	-0.058502	4.494144
290.501293	6929.019704	14.936448	-0.058458	4.491630
290.294378	6920.994947	14.941453	-0.058414	4.489115
290.307584	6913.082135	14.946458	-0.058411	4.486634
290.580765	6905.016892	14.951463	-0.058457	4.484105
290.555538	6897.066527	14.956467	-0.058447	4.481609
290.590931	6889.034509	14.961472	-0.058448	4.479087
290.423093	6881.042924	14.966477	-0.058412	4.476575
290.307423	6873.049382	14.971482	-0.058385	4.474062
290.244631	6864.993333	14.976487	-0.058368	4.471527
290.256656	6856.998565	14.981491	-0.058365	4.469011
290.276961	6849.040914	14.986496	-0.058364	4.466505
290.186124	6840.995903	14.991501	-0.058341	4.463970
290.176021	6833.035735	14.996506	-0.058334	4.461460
290.190631	6824.998637	15.001511	-0.058332	4.458925
290.289727	6817.074848	15.006515	-0.058345	4.456424
290.299269	6809.003398	15.011520	-0.058342	4.453875
290.048243	6801.006987	15.016525	-0.058290	4.451347
290.012773	6793.011507	15.021530	-0.058278	4.448819
289.907246	6785.001764	15.026535	-0.058253	4.446284
289.910965	6776.977464	15.031539	-0.058248	4.443744
289.895584	6769.035860	15.036544	-0.058240	4.441229
289.845643	6761.043097	15.041549	-0.058226	4.438696
289.803338	6753.039072	15.046554	-0.058213	4.436157
289.682246	6745.000410	15.051559	-0.058185	4.433606
289.646446	6736.934757	15.056563	-0.058173	4.431046
289.587094	6728.973364	15.061568	-0.058157	4.428517
289.689991	6720.936633	15.066573	-0.058171	4.425963
289.673967	6712.969058	15.071578	-0.058163	4.423429
289.578603	6704.960154	15.076583	-0.058140	4.420880
289.474095	6697.033498	15.081587	-0.058115	4.418356
289.460718	6688.975810	15.086592	-0.058107	4.415789
289.249684	6680.967966	15.091597	-0.058063	4.413236
289.323865	6672.954534	15.096602	-0.058071	4.410680
289.431292	6664.948134	15.101607	-0.058086	4.408126
289.529848	6656.968964	15.106611	-0.058099	4.405579
289.301569	6649.015291	15.111616	-0.058051	4.403036
289.171760	6640.967064	15.116621	-0.058022	4.400463
289.413596	6633.055041	15.121626	-0.058062	4.397933
289.256832	6624.961062	15.126631	-0.058027	4.395342
289.205863	6616.954928	15.131635	-0.058013	4.392778
289.212514	6608.916470	15.136640	-0.058009	4.390202
289.257877	6600.932686	15.141645	-0.058012	4.387643
289.182550	6592.984851	15.146650	-0.057993	4.385093
288.990019	6584.982496	15.151655	-0.057952	4.382523
289.020346	6576.968295	15.156659	-0.057952	4.379949
288.931839	6569.043505	15.161664	-0.057930	4.377402
288.809624	6560.981303	15.166669	-0.057902	4.374809
289.177983	6552.975985	15.171674	-0.057966	4.372236
288.786373	6544.920602	15.176679	-0.057888	4.369640
288.840410	6536.988686	15.181683	-0.057893	4.367085
288.889513	6528.961754	15.186688	-0.057896	4.364498
288.863726	6521.029078	15.191693	-0.057886	4.361940
288.785592	6513.015045	15.196698	-0.057867	4.359353
288.651410	6505.018508	15.201703	-0.057837	4.356770
288.845096	6496.971002	15.206707	-0.057867	4.354172
288.428132	6488.869022	15.211712	-0.057784	4.351550
288.395089	6480.898451	15.216717	-0.057773	4.348971
288.558914	6472.909321	15.221722	-0.057798	4.346387
288.558587	6464.903214	15.226727	-0.057793	4.343794
288.535292	6456.962088	15.231731	-0.057784	4.341220
288.624050	6448.982907	15.236736	-0.057795	4.338634
288.451762	6440.945688	15.241741	-0.057758	4.336025
288.287643	6432.954548	15.246746	-0.057722	4.333430
288.327453	6424.925435	15.251751	-0.057724	4.330822
288.391052	6416.948645	15.256755	-0.057731	4.328230
288.171723	6408.945405	15.261760	-0.057685	4.325625
288.031620	6400.949161	15.266765	-0.057653	4.323022
288.246646	6392.949858	15.271770	-0.057688	4.320419
288.193765	6384.966129	15.276775	-0.057673	4.317817
288.090801	6376.957744	15.281779	-0.057649	4.315206
288.244090	6368.939768	15.286784	-0.057672	4.312592
288.244148	6360.853649	15.291789	-0.057667	4.309952
288.170466	6352.967245	15.296794	-0.057648	4.307376
288.164190	6344.901599	15.301799	-0.057641	4.304740
288.122127	6336.948651	15.306803	-0.057628	4.302139
287.977082	6328.941951	15.311808	-0.057596	4.299518
288.061082	6320.929913	15.316813	-0.057607	4.296896
288.147689	6312.914103	15.321818	-0.057617	4.294270
287.975236	6304.916176	15.326823	-0.057580	4.291647
287.846848	6296.881214	15.331827	-0.057551	4.289011
288.033001	6288.942326	15.336832	-0.057580	4.286407
288.120152	6280.943201	15.341837	-0.057591	4.283780
287.915919	6272.945866	15.346842	-0.057548	4.281151
287.649409	6264.949426	15.351847	-0.057493	4.278519
287.651049	6256.898022	15.356851	-0.057488	4.275870
287.644749	6248.906805	15.361856	-0.057482	4.273239
287.533400	6240.838933	15.366861	-0.057456	4.270581
287.779693	6232.903102	15.371866	-0.057497	4.267967
287.563057	6224.856529	15.376871	-0.057451	4.265311
287.543738	6216.887355	15.381875	-0.057442	4.262681
287.647739	6208.901853	15.386880	-0.057456	4.260045
287.602985	6200.924332	15.391885	-0.057443	4.257408
287.330443	6192.929657	15.396890	-0.057387	4.254762
287.081904	6184.911116	15.401895	-0.057335	4.252107
287.436399	6176.907454	15.406899	-0.057396	4.249460
287.218997	6168.900033	15.411904	-0.057351	4.246806
287.056786	6160.880165	15.416909	-0.057315	4.244146
287.249769	6152.913733	15.421914	-0.057346	4.241505
287.115538	6144.901288	15.426919	-0.057316	4.238845
287.194873	6136.919790	15.431923	-0.057325	4.236195
287.194723	6128.915492	15.436928	-0.057320	4.233535
287.162692	6120.835500	15.441933	-0.057309	4.230848
287.212380	6112.911173	15.446938	-0.057313	4.228211
287.067708	6104.857802	15.451943	-0.057281	4.225529
287.074755	6096.923171	15.456947	-0.057277	4.222885
286.970908	6088.905059	15.461952	-0.057252	4.220211
286.819740	6080.933726	15.466957	-0.057219	4.217551
286.924120	6072.944839	15.471962	-0.057233	4.214885
287.021856	6064.922861	15.476967	-0.057246	4.212207
286.849415	6056.899249	15.481971	-0.057209	4.209523
286.747946	6048.995309	15.486976	-0.057185	4.206879
286.790180	6040.932467	15.491981	-0.057187	4.204181
286.944738	6032.978486	15.496986	-0.057211	4.201519
286.813636	6024.955522	15.501991	-0.057181	4.198830
286.642139	6016.953924	15.506995	-0.057144	4.196145
286.723301	6008.862084	15.512000	-0.057154	4.193431
286.449339	6000.816515	15.517005	-0.057098	4.190727
286.546205	5992.871218	15.522010	-0.057110	4.188059
286.512571	5984.837670	15.527015	-0.057099	4.185358
286.397550	5976.883414	15.532019	-0.057072	4.182682
286.421940	5968.903792	15.537024	-0.057072	4.179996
286.630952	5960.915826	15.542029	-0.057105	4.177308
286.567618	5952.879867	15.547034	-0.057088	4.174599
286.329671	5944.896600	15.552039	-0.057039	4.171904
286.365528	5936.874309	15.557043	-0.057040	4.169197
286.376526	5928.888556	15.562048	-0.057037	4.166501
286.316456	5920.878048	15.567053	-0.057021	4.163793
286.345615	5912.913135	15.572058	-0.057021	4.161101
286.124550	5904.919490	15.577063	-0.056975	4.158394
286.052748	5896.907582	15.582067	-0.056956	4.155680
286.013882	5888.894279	15.587072	-0.056944	4.152965
286.169551	5880.839893	15.592077	-0.056967	4.150236
286.264025	5872.889489	15.597082	-0.056980	4.147541
286.072998	5864.854036	15.602087	-0.056939	4.144811
286.020498	5856.896251	15.607091	-0.056924	4.142107
286.199573	5848.891389	15.612096	-0.056952	4.139388
285.701788	5840.946176	15.617101	-0.056854	4.136680
285.719823	5832.896155	15.622106	-0.056852	4.133941
285.661199	5824.861569	15.627111	-0.056836	4.131204
285.783998	5816.879786	15.632115	-0.056854	4.128485
285.622440	5808.898036	15.637120	-0.056818	4.125761
285.643593	5800.877430	15.642125	-0.056817	4.123024
285.759361	5792.876025	15.647130	-0.056834	4.120293
285.837666	5784.904107	15.652135	-0.056843	4.117570
285.647242	5776.913681	15.657139	-0.056802	4.114836
285.795892	5768.843891	15.662144	-0.056825	4.112077
285.573712	5760.824419	15.667149	-0.056778	4.109328
285.581830	5752.875480	15.672154	-0.056774	4.106605
285.532576	5744.888485	15.677159	-0.056760	4.103866
285.470470	5736.890966	15.682163	-0.056743	4.101121
285.314501	5728.921532	15.687168	-0.056709	4.098383
285.222499	5720.895065	15.692173	-0.056687	4.095625
285.382251	5712.864280	15.697178	-0.056711	4.092866
285.324152	5704.874566	15.702183	-0.056695	4.090117
285.219023	5696.885752	15.707187	-0.056670	4.087365
285.257206	5688.887663	15.712192	-0.056672	4.084611
285.184945	5680.931928	15.717197	-0.056654	4.081867
285.154639	5672.958194	15.722202	-0.056643	4.079117
285.181401	5664.959547	15.727207	-0.056642	4.076356
285.191533	5656.921804	15.732211	-0.056639	4.073580
285.145231	5648.899948	15.737216	-0.056625	4.070807
285.150344	5640.911277	15.742221	-0.056621	4.068044
285.206468	5632.907024	15.747226	-0.056626	4.065274
285.012656	5624.956290	15.752231	-0.056585	4.062518
284.993907	5616.929096	15.757235	-0.056576	4.059736
285.007108	5609.002387	15.762240	-0.056574	4.056987
284.754205	5600.928436	15.767245	-0.056521	4.054181
284.701946	5592.931796	15.772250	-0.056506	4.051403
284.680451	5584.910643	15.777255	-0.056497	4.048615
284.790051	5576.882332	15.782259	-0.056512	4.045825
284.514646	5568.957415	15.787264	-0.056456	4.043063
284.541430	5560.914966	15.792269	-0.056455	4.040262
284.717210	5552.953223	15.797274	-0.056483	4.037490
284.538499	5544.939594	15.802279	-0.056444	4.034693
284.457009	5536.813841	15.807283	-0.056424	4.031856
284.644890	5528.852884	15.812288	-0.056454	4.029078
284.469087	5520.876536	15.817293	-0.056416	4.026288
284.436027	5512.911168	15.822298	-0.056404	4.023502
284.351893	5504.926824	15.827303	-0.056384	4.020707
284.502311	5496.920812	15.832307	-0.056406	4.017905
284.357549	5488.908449	15.837312	-0.056374	4.015095
284.189705	5480.888551	15.842317	-0.056338	4.012280
284.307163	5472.875856	15.847322	-0.056354	4.009470
284.287672	5464.918420	15.852327	-0.056346	4.006675
284.091259	5456.872388	15.857331	-0.056304	4.003845
284.384847	5448.927128	15.862336	-0.056353	4.001055
284.262316	5440.910406	15.867341	-0.056325	3.998232
284.148901	5432.938869	15.872346	-0.056299	3.995423
284.025467	5424.895522	15.877351	-0.056271	3.992586
284.226333	5416.847465	15.882355	-0.056303	3.989751
284.185750	5408.905514	15.887360	-0.056290	3.986947
284.071857	5400.913365	15.892365	-0.056264	3.984123
284.031739	5392.965890	15.897370	-0.056251	3.981313
284.231780	5384.913991	15.902375	-0.056283	3.978469
284.064554	5376.912350	15.907379	-0.056247	3.975634
284.145146	5368.923315	15.912384	-0.056256	3.972806
284.128456	5360.876748	15.917389	-0.056248	3.969954
283.947546	5352.944969	15.922394	-0.056209	3.967137
283.824484	5344.929977	15.927399	-0.056181	3.964290
283.735249	5336.958720	15.932403	-0.056159	3.961457
283.887517	5328.978080	15.937408	-0.056182	3.958623
283.701894	5320.940455	15.942413	-0.056143	3.955761
283.657417	5312.921176	15.947418	-0.056129	3.952906
283.707576	5304.914499	15.952423	-0.056133	3.950054
283.532989	5296.920198	15.957427	-0.056095	3.947201
283.783580	5288.961632	15.962432	-0.056137	3.944367
283.670049	5280.955818	15.967437	-0.056111	3.941507
283.581698	5272.993935	15.972442	-0.056089	3.938661
283.420467	5264.978619	15.977447	-0.056054	3.935792
283.501922	5256.952763	15.982451	-0.056064	3.932922
283.647206	5248.953951	15.987456	-0.056085	3.930061
283.374920	5240.998434	15.992461	-0.056030	3.927205
283.558297	5232.991904	15.997466	-0.056058	3.924338
283.475374	5225.021160	16.002471	-0.056038	3.921476
283.237703	5216.996349	16.007475	-0.055988	3.918590
283.172881	5209.011297	16.012480	-0.055971	3.915719
283.260519	5200.962713	16.017485	-0.055982	3.912827
283.103926	5192.962088	16.022490	-0.055948	3.909944
283.092566	5185.009336	16.027495	-0.055940	3.907080
283.101280	5176.957481	16.032499	-0.055937	3.904178
283.118381	5169.024527	16.037504	-0.055935	3.901317
282.936609	5160.979804	16.042509	-0.055896	3.898410
282.950762	5152.998297	16.047514	-0.055893	3.895527
282.975790	5144.971192	16.052519	-0.055893	3.892626
282.870303	5136.950051	16.057523	-0.055868	3.889722
282.887496	5129.043106	16.062528	-0.055866	3.886860
282.795916	5120.985823	16.067533	-0.055843	3.883939
282.757917	5113.009257	16.072538	-0.055831	3.881046
282.768828	5105.003359	16.077543	-0.055828	3.878141
282.833943	5097.020318	16.082547	-0.055835	3.875244
282.846887	5088.822751	16.087552	-0.055832	3.872265
282.646286	5080.790647	16.092557	-0.055789	3.869340
282.841720	5072.887263	16.097562	-0.055821	3.866467
282.767590	5064.941814	16.102567	-0.055802	3.863572
282.905670	5056.942807	16.107571	-0.055822	3.860659
282.833614	5048.980995	16.112576	-0.055804	3.857754
282.709495	5040.953708	16.117581	-0.055775	3.854821
282.647087	5032.997521	16.122586	-0.055758	3.851913
282.650610	5024.961772	16.127591	-0.055754	3.848975
282.487799	5016.971274	16.132595	-0.055718	3.846048
282.515683	5009.018901	16.137600	-0.055718	3.843137
282.324129	5001.014158	16.142605	-0.055677	3.840200
282.350242	4993.058703	16.147610	-0.055677	3.837283
282.354323	4985.005943	16.152615	-0.055673	3.834328
282.384840	4976.974893	16.157619	-0.055673	3.831379
282.503168	4969.012954	16.162624	-0.055690	3.828454
282.451293	4961.033670	16.167629	-0.055675	3.825518
282.337999	4953.072531	16.172634	-0.055649	3.822585
282.253346	4945.026970	16.177639	-0.055628	3.819619
282.391067	4937.078160	16.182643	-0.055648	3.816691
282.404342	4929.070696	16.187648	-0.055645	3.813737
282.309136	4921.053753	16.192653	-0.055622	3.810775
282.146275	4913.085028	16.197658	-0.055587	3.807826
282.200015	4905.050845	16.202663	-0.055592	3.804856
281.984396	4897.117947	16.207667	-0.055546	3.801915
282.055520	4889.101987	16.212672	-0.055554	3.798947
282.128150	4881.112382	16.217677	-0.055563	3.795987
282.026890	4873.073656	16.222682	-0.055539	3.793002
281.896181	4865.050620	16.227687	-0.055509	3.790020
281.786158	4857.052886	16.232691	-0.055483	3.787046
282.046442	4849.079658	16.237696	-0.055527	3.784087
281.987657	4841.038599	16.242701	-0.055510	3.781093
281.892702	4833.099955	16.247706	-0.055488	3.778134
281.890252	4825.064048	16.252711	-0.055482	3.775138
281.561378	4817.086061	16.257715	-0.055415	3.772154
281.599714	4809.111476	16.262720	-0.055417	3.769178
281.595087	4801.053925	16.267725	-0.055411	3.766167
281.591802	4793.092038	16.272730	-0.055405	3.763190
281.367768	4785.108291	16.277735	-0.055358	3.760197
281.312340	4777.133973	16.282739	-0.055343	3.757208
281.482106	4769.123841	16.287744	-0.055369	3.754210
281.419147	4761.062893	16.292749	-0.055352	3.751184
281.505386	4753.084840	16.297754	-0.055363	3.748191
281.496628	4745.070039	16.302759	-0.055356	3.745179
281.549613	4737.116762	16.307763	-0.055361	3.742189
281.321330	4729.141829	16.312768	-0.055313	3.739183
281.226227	4721.132740	16.317773	-0.055290	3.736164
281.311859	4713.141137	16.322778	-0.055301	3.733153
281.110640	4705.143472	16.327783	-0.055258	3.730131
281.113629	4697.132827	16.332787	-0.055254	3.727106
281.178797	4689.142078	16.337792	-0.055261	3.724088
281.340121	4681.186309	16.342797	-0.055286	3.721083
281.089604	4673.201409	16.347802	-0.055234	3.718055
280.981414	4665.204114	16.352807	-0.055208	3.715023
280.792982	4657.100856	16.357811	-0.055168	3.711946
280.928870	4649.092036	16.362816	-0.055188	3.708911
280.684534	4641.122554	16.367821	-0.055137	3.705878
280.878529	4633.173942	16.372826	-0.055168	3.702862
280.805468	4625.154771	16.377831	-0.055149	3.699810
280.692914	4617.176805	16.382835	-0.055123	3.696770
280.755561	4609.172683	16.387840	-0.055130	3.693722
280.555541	4601.198953	16.392845	-0.055087	3.690677
280.490139	4593.207491	16.397850	-0.055070	3.687625
280.579179	4585.169983	16.402855	-0.055081	3.684558
280.556973	4577.224882	16.407859	-0.055072	3.681520
280.664212	4569.257357	16.412864	-0.055087	3.678474
280.415252	4561.239452	16.417869	-0.055035	3.675398
280.376381	4553.220028	16.422874	-0.055023	3.672324
280.498263	4545.193308	16.427879	-0.055040	3.669248
280.188954	4537.224221	16.432883	-0.054977	3.666181
280.519324	4529.219610	16.437888	-0.055034	3.663114
280.348449	4521.242483	16.442893	-0.054997	3.660043
280.401981	4513.267454	16.447898	-0.055001	3.656975
280.447442	4505.255895	16.452903	-0.055005	3.653890
280.367193	4497.202186	16.457907	-0.054984	3.650784
280.150717	4489.244771	16.462912	-0.054939	3.647708
280.058840	4481.227434	16.467917	-0.054917	3.644610
280.072692	4473.294471	16.472922	-0.054914	3.641544
280.301222	4465.276729	16.477927	-0.054951	3.638449
279.905141	4457.293616	16.482931	-0.054872	3.635348
280.155098	4449.246899	16.487936	-0.054914	3.632237
280.003268	4441.255044	16.492941	-0.054880	3.629134
279.980846	4433.244185	16.497946	-0.054871	3.626024
279.897934	4425.262923	16.502951	-0.054850	3.622921
279.743149	4417.247031	16.507955	-0.054816	3.619800
279.832025	4409.316417	16.512960	-0.054827	3.616717
279.736483	4401.290960	16.517965	-0.054804	3.613589
279.887467	4393.265470	16.522970	-0.054827	3.610464
279.811789	4385.305337	16.527975	-0.054808	3.607357
279.683039	4377.321512	16.532979	-0.054779	3.604236
279.806576	4369.345837	16.537984	-0.054797	3.601122
279.721784	4361.377548	16.542989	-0.054776	3.598003
279.647895	4353.377966	16.547994	-0.054757	3.594869
279.652653	4345.348685	16.552999	-0.054752	3.591723
279.708472	4337.304460	16.558003	-0.054757	3.588570
279.380219	4329.380910	16.563008	-0.054691	3.585450
279.161557	4321.419133	16.568013	-0.054645	3.582316
279.438302	4313.391125	16.573018	-0.054692	3.579167
279.548042	4305.420293	16.578023	-0.054707	3.576033
279.349193	4297.381505	16.583027	-0.054664	3.572861
279.280766	4289.378392	16.588032	-0.054647	3.569704
279.293561	4281.403318	16.593037	-0.054644	3.566557
279.184276	4273.411878	16.598042	-0.054618	3.563398
279.041606	4265.437939	16.603047	-0.054586	3.560241
279.123565	4257.432429	16.608051	-0.054596	3.557076
279.157760	4249.421010	16.613056	-0.054598	3.553905
278.855185	4241.309529	16.618061	-0.054536	3.550681
278.968563	4233.369596	16.623066	-0.054552	3.547534
278.943003	4225.379469	16.628071	-0.054542	3.544360
278.781949	4217.418454	16.633075	-0.054507	3.541191
278.801823	4209.426721	16.638080	-0.054505	3.538013
278.752178	4201.416841	16.643085	-0.054491	3.534822
278.726318	4193.422602	16.648090	-0.054481	3.531636
278.621155	4185.436129	16.653095	-0.054456	3.528447
278.505709	4177.431134	16.658099	-0.054429	3.525247
278.625107	4169.485082	16.663104	-0.054446	3.522076
278.490321	4161.489084	16.668109	-0.054416	3.518874
278.433528	4153.515509	16.673114	-0.054400	3.515680
278.634083	4145.466381	16.678119	-0.054432	3.512461
278.343396	4137.453777	16.683123	-0.054373	3.509238
278.357455	4129.484248	16.688128	-0.054370	3.506039
278.496172	4121.505363	16.693133	-0.054391	3.502838
278.514786	4113.514315	16.698138	-0.054389	3.499625
278.386106	4105.555226	16.703143	-0.054360	3.496417
278.399167	4097.526632	16.708147	-0.054357	3.493182
278.466681	4089.516697	16.713152	-0.054365	3.489954
278.247875	4081.565937	16.718157	-0.054319	3.486738
278.275223	4073.564684	16.723162	-0.054319	3.483506
278.260130	4065.585763	16.728167	-0.054310	3.480279
278.085351	4057.623764	16.733171	-0.054273	3.477050
278.133105	4049.593118	16.738176	-0.054276	3.473798
278.124798	4041.539023	16.743181	-0.054270	3.470532
278.138982	4033.556077	16.748186	-0.054267	3.467291
278.117807	4025.585711	16.753191	-0.054258	3.464052
278.030421	4017.602779	16.758195	-0.054236	3.460803
277.996170	4009.633104	16.763200	-0.054225	3.457558
277.804854	4001.613071	16.768205	-0.054184	3.454284
277.733332	3993.610998	16.773210	-0.054165	3.451018
277.851454	3985.618069	16.778215	-0.054182	3.447759
277.790187	3977.605138	16.783219	-0.054166	3.444482
277.879508	3969.674647	16.788224	-0.054177	3.441242
277.720098	3961.670404	16.793229	-0.054142	3.437960
277.689919	3953.660322	16.798234	-0.054131	3.434676
277.789528	3945.657222	16.803239	-0.054145	3.431397
277.616948	3937.628502	16.808243	-0.054107	3.428095
277.868858	3929.637357	16.813248	-0.054149	3.424819
277.717426	3921.681567	16.818253	-0.054116	3.421541
277.580421	3913.713343	16.823258	-0.054085	3.418256
277.569071	3905.712949	16.828263	-0.054078	3.414958
277.616518	3897.695008	16.833267	-0.054081	3.411652
277.464380	3889.731597	16.838272	-0.054048	3.408358
277.344084	3881.734812	16.843277	-0.054020	3.405048
277.447717	3873.757376	16.848282	-0.054034	3.401751
277.250729	3865.815746	16.853287	-0.053992	3.398455
277.237618	3857.786739	16.858291	-0.053985	3.395126
277.357928	3849.677726	16.863296	-0.054002	3.391766
277.144920	3841.709895	16.868301	-0.053957	3.388448
276.962278	3833.733904	16.873306	-0.053918	3.385126
277.195745	3825.765175	16.878311	-0.053956	3.381817
277.328512	3817.757237	16.883315	-0.053975	3.378486
277.166084	3809.806881	16.888320	-0.053940	3.375165
277.136612	3801.804535	16.893325	-0.053929	3.371823
276.979846	3793.815762	16.898330	-0.053895	3.368479
276.924698	3785.828557	16.903335	-0.053879	3.365137
276.913177	3777.854527	16.908339	-0.053872	3.361798
276.890270	3769.877492	16.913344	-0.053863	3.358454
276.766262	3761.885874	16.918349	-0.053834	3.355097
276.701653	3753.854842	16.923354	-0.053817	3.351722
276.685676	3745.858910	16.928359	-0.053809	3.348360
276.600567	3737.839186	16.933363	-0.053788	3.344982
276.646841	3729.902141	16.938368	-0.053791	3.341641
276.485448	3721.903010	16.943373	-0.053756	3.338262
276.606415	3713.920714	16.948378	-0.053773	3.334898
276.562034	3705.918768	16.953383	-0.053760	3.331515
276.559613	3697.882194	16.958387	-0.053754	3.328116
276.731973	3689.901887	16.963392	-0.053781	3.324744
276.651048	3681.973964	16.968397	-0.053761	3.321382
276.411460	3673.973207	16.973402	-0.053711	3.317979
276.282673	3666.006995	16.978407	-0.053682	3.314591
276.183137	3657.947306	16.983411	-0.053658	3.311161
276.227689	3649.948499	16.988416	-0.053661	3.307759
276.250229	3641.951072	16.993421	-0.053660	3.304353
276.194973	3634.009795	16.998426	-0.053644	3.300965
276.144855	3626.060161	17.003431	-0.053630	3.297570
276.080566	3618.027265	17.008435	-0.053613	3.294135
276.065035	3610.023943	17.013440	-0.053605	3.290711
275.846302	3602.052326	17.018445	-0.053559	3.287289
275.785928	3594.053744	17.023450	-0.053542	3.283859
275.855368	3586.099833	17.028455	-0.053550	3.280448
276.181660	3578.085162	17.033459	-0.053606	3.277019
275.811170	3570.125925	17.038464	-0.053531	3.273582
275.601096	3562.083089	17.043469	-0.053487	3.270112
275.714739	3554.104877	17.048474	-0.053503	3.266678
275.803116	3546.122115	17.053479	-0.053514	3.263239
275.655101	3538.110809	17.058483	-0.053481	3.259774
275.793703	3530.180014	17.063488	-0.053502	3.256351
275.616319	3522.138675	17.068493	-0.053464	3.252864
275.563633	3514.121949	17.073498	-0.053449	3.249389
275.544070	3506.184889	17.078503	-0.053440	3.245947
275.437214	3498.188134	17.083507	-0.053415	3.242471
275.528278	3490.208971	17.088512	-0.053427	3.239007
275.326799	3482.233167	17.093517	-0.053384	3.235529
275.342876	3474.173450	17.098522	-0.053382	3.232020
275.409087	3466.176500	17.103527	-0.053389	3.228536
275.422637	3458.150174	17.108531	-0.053386	3.225033
275.360970	3450.236726	17.113536	-0.053369	3.221573
275.222853	3442.249093	17.118541	-0.053338	3.218074
275.399568	3434.229957	17.123546	-0.053366	3.214570
275.269407	3426.259757	17.128551	-0.053337	3.211071
275.081382	3418.257552	17.133555	-0.053296	3.207551
275.349874	3410.289263	17.138560	-0.053341	3.204062
275.161355	3402.330950	17.143565	-0.053301	3.200554
274.973377	3394.375027	17.148570	-0.053261	3.197043
275.026943	3386.360371	17.153575	-0.053265	3.193513
274.823174	3378.335233	17.158579	-0.053222	3.189963
274.989295	3370.348797	17.163584	-0.053248	3.186442
274.909169	3362.379854	17.168589	-0.053228	3.182914
274.714940	3354.383506	17.173594	-0.053186	3.179366
274.865522	3346.427829	17.178599	-0.053209	3.175846
274.818603	3338.395133	17.183603	-0.053195	3.172280
274.830715	3330.412865	17.188608	-0.053192	3.168735
274.584374	3322.439947	17.193613	-0.053141	3.165178
274.615151	3314.461895	17.198618	-0.053142	3.161628
274.710106	3306.471167	17.203623	-0.053154	3.158070
274.528896	3298.490374	17.208627	-0.053115	3.154501
274.568057	3290.467206	17.213632	-0.053117	3.150919
274.595873	3282.474486	17.218637	-0.053117	3.147345
274.636870	3274.458184	17.223642	-0.053120	3.143758
274.635126	3266.519939	17.228647	-0.053114	3.140199
274.541349	3258.536460	17.233651	-0.053092	3.136612
274.681400	3250.543328	17.238656	-0.053113	3.133027
274.382853	3242.553257	17.243661	-0.053052	3.129420
274.297638	3234.586126	17.248666	-0.053031	3.125829
274.287431	3226.640846	17.253671	-0.053024	3.122246
274.072929	3218.635772	17.258675	-0.052978	3.118623
274.220824	3210.646918	17.263680	-0.053001	3.115020
274.185019	3202.627589	17.268685	-0.052989	3.111390
274.107188	3194.623896	17.273690	-0.052969	3.107762
274.013414	3186.669718	17.278695	-0.052946	3.104150
273.914364	3178.665581	17.283699	-0.052923	3.100512
274.102992	3170.685970	17.288704	-0.052953	3.096894
273.979856	3162.722241	17.293709	-0.052925	3.093264
273.889355	3154.693415	17.298714	-0.052903	3.089602
274.079626	3146.738174	17.303719	-0.052933	3.085982
274.021608	3138.755097	17.308723	-0.052917	3.082334
273.878523	3130.779882	17.313728	-0.052885	3.078680
273.879254	3122.808476	17.318733	-0.052880	3.075032
273.799749	3114.721938	17.323738	-0.052860	3.071322
273.742705	3106.744920	17.328743	-0.052844	3.067659
273.537200	3098.766803	17.333747	-0.052800	3.063984
273.679273	3090.794710	17.338752	-0.052822	3.060323
273.451216	3082.859836	17.343757	-0.052774	3.056659
273.468617	3074.841058	17.348762	-0.052772	3.052962
273.576047	3066.841654	17.353767	-0.052787	3.049274
273.338922	3058.870491	17.358771	-0.052738	3.045579
273.505805	3050.913279	17.363776	-0.052763	3.041905
273.445919	3042.932478	17.368781	-0.052747	3.038204
273.370797	3034.940815	17.373786	-0.052728	3.034493
273.529761	3026.925941	17.378791	-0.052752	3.030778
273.253415	3018.962721	17.383795	-0.052696	3.027062
273.340345	3010.974263	17.388800	-0.052707	3.023347
273.258266	3002.994479	17.393805	-0.052686	3.019623
273.223262	2995.023003	17.398810	-0.052674	3.015900
273.353958	2987.015324	17.403815	-0.052693	3.012165
273.181913	2979.035947	17.408819	-0.052656	3.008423
273.031368	2971.066325	17.413824	-0.052623	3.004682
273.010383	2963.116344	17.418829	-0.052614	3.000951
273.045158	2955.103943	17.423834	-0.052615	2.997190
273.006502	2947.127925	17.428839	-0.052603	2.993437
273.121174	2939.080089	17.433843	-0.052619	2.989654
273.085532	2931.133778	17.438848	-0.052607	2.985906
272.846464	2923.171496	17.443853	-0.052557	2.982135
272.833017	2915.163698	17.448858	-0.052550	2.978350
272.960644	2907.209717	17.453863	-0.052568	2.974592
272.791866	2899.209823	17.458867	-0.052532	2.970793
272.658728	2891.251948	17.463872	-0.052502	2.967011
272.803138	2883.248251	17.468877	-0.052523	2.963216
272.791404	2875.260360	17.473882	-0.052516	2.959416
272.658751	2867.328506	17.478887	-0.052486	2.955631
272.560762	2859.283418	17.483891	-0.052462	2.951790
272.643098	2851.305168	17.488896	-0.052473	2.947984
272.613236	2843.316693	17.493901	-0.052462	2.944163
272.628806	2835.342152	17.498906	-0.052459	2.940346
272.579386	2827.402590	17.503911	-0.052445	2.936538
272.453505	2819.399773	17.508915	-0.052416	2.932690
272.412039	2811.410661	17.513920	-0.052404	2.928848
272.330895	2803.433145	17.518925	-0.052383	2.925005
272.403382	2795.454534	17.523930	-0.052392	2.921164
272.393422	2787.513518	17.528935	-0.052384	2.917331
272.229084	2779.472678	17.533939	-0.052349	2.913438
272.062099	2771.432005	17.538944	-0.052312	2.909539
272.214552	2763.450733	17.543949	-0.052335	2.905680
272.254913	2755.489135	17.548954	-0.052338	2.901820
271.976709	2747.577819	17.553959	-0.052281	2.897962
272.001888	2739.552510	17.558963	-0.052280	2.894060
272.045772	2731.564763	17.563968	-0.052283	2.890172
271.906943	2723.601007	17.568973	-0.052252	2.886280
271.984933	2715.614350	17.573978	-0.052262	2.882384
271.890278	2707.687048	17.578983	-0.052239	2.878502
271.790408	2699.700354	17.583987	-0.052215	2.874585
271.811807	2691.669677	17.588992	-0.052214	2.870649
271.934738	2683.679922	17.593997	-0.052231	2.866732
271.803127	2675.720081	17.599002	-0.052202	2.862811
271.755671	2667.773158	17.604007	-0.052188	2.858895
271.704970	2659.772973	17.609011	-0.052173	2.854948
271.509626	2651.810946	17.614016	-0.052131	2.851006
271.420502	2643.830362	17.619021	-0.052110	2.847055
271.394930	2635.843625	17.624026	-0.052100	2.843099
271.540196	2627.880102	17.629031	-0.052121	2.839159
271.181416	2619.928274	17.634035	-0.052049	2.835190
271.376054	2611.878355	17.639040	-0.052080	2.831199
271.378459	2603.899818	17.644045	-0.052076	2.827226
271.206498	2595.933636	17.649050	-0.052039	2.823244
271.114900	2587.993960	17.654055	-0.052016	2.819275
271.268421	2579.976907	17.659059	-0.052040	2.815275
271.151823	2571.994068	17.664064	-0.052013	2.811271
271.182241	2564.028782	17.669069	-0.052013	2.807279
271.182363	2556.029219	17.674074	-0.052008	2.803261
271.164813	2548.078522	17.679079	-0.052000	2.799262
271.083439	2540.121792	17.684083	-0.051979	2.795250
271.054683	2532.124044	17.689088	-0.051969	2.791215
271.131643	2524.125002	17.694093	-0.051978	2.787180
270.996239	2516.163398	17.699098	-0.051947	2.783145
270.950434	2508.216540	17.704103	-0.051934	2.779117
270.921871	2500.231249	17.709107	-0.051923	2.775064
270.661217	2492.253404	17.714112	-0.051869	2.770996
270.609072	2484.283893	17.719117	-0.051854	2.766939
270.690726	2476.290839	17.724122	-0.051864	2.762871
270.880874	2468.296174	17.729127	-0.051895	2.758803
270.775409	2460.350974	17.734131	-0.051870	2.754736
270.776655	2452.269679	17.739136	-0.051865	2.750601
270.832046	2444.295192	17.744141	-0.051870	2.746517
270.586441	2436.358952	17.749146	-0.051819	2.742428
270.677538	2428.400330	17.754151	-0.051831	2.738343
270.610952	2420.440095	17.759155	-0.051813	2.734240
270.364550	2412.469613	17.764160	-0.051762	2.730115
270.375633	2404.497028	17.769165	-0.051759	2.725999
270.390462	2396.509490	17.774170	-0.051756	2.721869
270.446684	2388.552018	17.779175	-0.051762	2.717751
270.305465	2380.582642	17.784179	-0.051730	2.713608
270.425298	2372.549858	17.789184	-0.051747	2.709442
270.528006	2364.604553	17.794189	-0.051761	2.705314
270.237881	2356.663377	17.799194	-0.051702	2.701157
270.192192	2348.705809	17.804199	-0.051688	2.697001
269.932688	2340.728980	17.809203	-0.051635	2.692815
270.113435	2332.725328	17.814208	-0.051663	2.688636
269.831219	2324.785160	17.819213	-0.051606	2.684454
269.968202	2316.792567	17.824218	-0.051626	2.680265
270.279827	2308.821476	17.829223	-0.051679	2.676092
269.910053	2300.852355	17.834227	-0.051605	2.671869
269.506201	2292.903730	17.839232	-0.051524	2.667649
269.720860	2284.882003	17.844237	-0.051559	2.663423
269.465928	2276.938381	17.849242	-0.051506	2.659202
269.476324	2268.975119	17.854247	-0.051503	2.654980
269.456209	2260.971267	17.859251	-0.051494	2.650728
269.536947	2252.985505	17.864256	-0.051504	2.646486
269.491702	2245.035860	17.869261	-0.051490	2.642247
269.390397	2237.084837	17.874266	-0.051466	2.637998
269.448677	2229.108364	17.879271	-0.051472	2.633738
269.348929	2221.101598	17.884275	-0.051448	2.629445
269.182110	2213.163364	17.889280	-0.051412	2.625178
269.254300	2205.194641	17.894285	-0.051420	2.620902
269.216171	2197.225284	17.899290	-0.051408	2.616612
269.144754	2189.253173	17.904295	-0.051389	2.612312
269.071215	2181.265885	17.909299	-0.051370	2.607995
269.359270	2173.262448	17.914304	-0.051419	2.603688
269.093787	2165.354595	17.919309	-0.051364	2.599387
269.188512	2157.377073	17.924314	-0.051377	2.595066
269.098771	2149.236053	17.929319	-0.051355	2.590637
268.854742	2141.291083	17.934323	-0.051304	2.586296
268.672048	2133.367350	17.939328	-0.051265	2.581963
268.862081	2125.405361	17.944333	-0.051295	2.577628
268.860043	2117.439179	17.949338	-0.051289	2.573270
268.716870	2109.503982	17.954343	-0.051258	2.568912
268.656031	2101.518527	17.959347	-0.051241	2.564524
268.732175	2093.580235	17.964352	-0.051250	2.560165
268.817258	2085.633046	17.969357	-0.051261	2.555793
268.608411	2077.644210	17.974362	-0.051217	2.551371
268.558702	2069.674828	17.979367	-0.051202	2.546963
268.384292	2061.719625	17.984371	-0.051165	2.542546
268.583258	2053.742903	17.989376	-0.051196	2.538136
268.448187	2045.805946	17.994381	-0.051166	2.533717
268.402338	2037.819118	17.999386	-0.051152	2.529269
268.302511	2029.872567	18.004391	-0.051129	2.524831
268.302538	2021.907427	18.009395	-0.051123	2.520382
268.299231	2013.952033	18.014400	-0.051118	2.515931
268.123366	2005.970832	18.019405	-0.051080	2.511445
267.912351	1997.979909	18.024410	-0.051035	2.506943
268.191872	1990.012066	18.029415	-0.051082	2.502481
267.983991	1982.083790	18.034419	-0.051038	2.497998
267.859111	1974.116873	18.039424	-0.051010	2.493491
267.917754	1966.126614	18.044429	-0.051015	2.488976
267.877431	1958.155380	18.049434	-0.051003	2.484457
267.862882	1950.230492	18.054439	-0.050995	2.479958
267.767661	1942.277820	18.059443	-0.050972	2.475428
267.744782	1934.270385	18.064448	-0.050962	2.470865
267.891804	1926.298770	18.069453	-0.050985	2.466326
267.641386	1918.360629	18.074458	-0.050933	2.461768
267.662190	1910.410036	18.079463	-0.050931	2.457215
267.708107	1902.432829	18.084467	-0.050935	2.452640
267.453687	1894.492504	18.089472	-0.050882	2.448055
267.420269	1886.539532	18.094477	-0.050871	2.443471
267.623911	1878.551670	18.099482	-0.050903	2.438876
267.561375	1870.609476	18.104487	-0.050887	2.434278
267.361373	1862.570981	18.109491	-0.050844	2.429606
267.420654	1854.607841	18.114496	-0.050850	2.424988
267.426551	1846.672251	18.119501	-0.050846	2.420373
267.089895	1838.761846	18.124506	-0.050778	2.415738
267.053615	1830.788240	18.129511	-0.050766	2.411080
266.929272	1822.825231	18.134515	-0.050738	2.406412
266.927122	1814.868399	18.139520	-0.050732	2.401748
267.120698	1806.904381	18.144525	-0.050763	2.397087
267.231013	1798.904019	18.149530	-0.050778	2.392388
267.192066	1790.958820	18.154535	-0.050766	2.387701
266.877425	1783.038683	18.159539	-0.050702	2.382998
266.930517	1775.084821	18.164544	-0.050707	2.378294
267.003153	1767.115890	18.169549	-0.050715	2.373574
266.852846	1759.145486	18.174554	-0.050682	2.368826
266.777500	1751.203060	18.179559	-0.050663	2.364091
266.857126	1743.235567	18.184563	-0.050672	2.359343
266.679919	1735.331244	18.189568	-0.050634	2.354604
266.663479	1727.325407	18.194573	-0.050626	2.349807
266.598098	1719.357614	18.199578	-0.050609	2.345019
266.545820	1711.441164	18.204583	-0.050594	2.340253
266.487723	1703.480854	18.209587	-0.050578	2.335450
266.373306	1695.511038	18.214592	-0.050551	2.330627
266.552658	1687.546900	18.219597	-0.050579	2.325822
266.264670	1679.631444	18.224602	-0.050521	2.320998
266.357633	1671.693439	18.229607	-0.050533	2.316181
266.347919	1663.689380	18.234611	-0.050526	2.311306
266.294458	1655.736811	18.239616	-0.050511	2.306448
266.334470	1647.784889	18.244621	-0.050513	2.301588
266.266624	1639.840364	18.249626	-0.050495	2.296714
266.134416	1631.908640	18.254631	-0.050465	2.291831
266.058491	1623.936997	18.259635	-0.050446	2.286918
265.859121	1616.017495	18.264640	-0.050404	2.282016
266.093342	1608.065351	18.269645	-0.050442	2.277120
265.814598	1600.083769	18.274650	-0.050385	2.272152
266.001266	1592.072707	18.279655	-0.050415	2.267195
265.971171	1584.128381	18.284659	-0.050404	2.262249
265.785489	1576.220036	18.289664	-0.050364	2.257302
265.803464	1568.269389	18.294669	-0.050362	2.252334
265.653182	1560.314371	18.299674	-0.050329	2.247339
265.882165	1552.354308	18.304679	-0.050366	2.242362
265.668395	1544.447040	18.309683	-0.050321	2.237369
265.502882	1536.502343	18.314688	-0.050285	2.232345
265.699029	1528.515129	18.319693	-0.050317	2.227315
265.494434	1520.591156	18.324698	-0.050274	2.222278
265.409355	1512.674885	18.329703	-0.050252	2.217245
265.400674	1504.705365	18.334707	-0.050246	2.212173
265.359818	1496.751549	18.339712	-0.050233	2.207097
265.414615	1488.812075	18.344717	-0.050238	2.202027
265.286731	1480.894958	18.349722	-0.050209	2.196943
265.376608	1472.918116	18.354727	-0.050220	2.191829
265.195077	1464.961408	18.359731	-0.050181	2.186691
265.039772	1457.042030	18.364736	-0.050147	2.181567
265.275991	1449.080239	18.369741	-0.050186	2.176440
265.172047	1441.127401	18.374746	-0.050162	2.171275
265.042083	1433.213322	18.379751	-0.050132	2.166121
265.096766	1425.268866	18.384755	-0.050137	2.160951
264.920729	1417.359568	18.389760	-0.050099	2.155771
264.802200	1409.419247	18.394765	-0.050072	2.150563
264.753429	1401.444046	18.399770	-0.050058	2.145326
264.853867	1393.511052	18.404775	-0.050071	2.140119
264.760525	1385.590313	18.409779	-0.050049	2.134888
264.571585	1377.647331	18.414784	-0.050008	2.129620
264.729977	1369.705928	18.419789	-0.050033	2.124374
264.600940	1361.781511	18.424794	-0.050004	2.119098
264.552871	1353.852581	18.429799	-0.049989	2.113814
264.522005	1345.836608	18.434803	-0.049978	2.108461
264.437039	1337.918012	18.439808	-0.049957	2.103153
264.446954	1329.994786	18.444813	-0.049954	2.097839
264.329482	1322.066969	18.449818	-0.049927	2.092495
264.474979	1314.104646	18.454823	-0.049949	2.087140
264.305356	1306.204057	18.459827	-0.049912	2.081782
264.147896	1298.301213	18.464832	-0.049878	2.076410
264.376328	1290.319086	18.469837	-0.049915	2.071008
264.159117	1282.391741	18.474842	-0.049869	2.065585
264.017637	1274.496883	18.479847	-0.049838	2.060177
264.035724	1266.574225	18.484851	-0.049836	2.054753
264.207538	1258.585460	18.489856	-0.049863	2.049283
263.997023	1250.706107	18.494861	-0.049819	2.043836
263.942079	1242.780564	18.499866	-0.049803	2.038359
263.892754	1234.866285	18.504871	-0.049789	2.032875
263.690357	1226.920694	18.509875	-0.049746	2.027338
263.708768	1218.980052	18.514880	-0.049744	2.021813
263.773764	1211.060899	18.519885	-0.049751	2.016292
263.696540	1203.116012	18.524890	-0.049732	2.010723
263.603373	1195.205082	18.529895	-0.049709	2.005161
263.627712	1187.277688	18.534899	-0.049709	1.999584
263.603622	1179.369172	18.539904	-0.049699	1.994000
263.551758	1171.431869	18.544909	-0.049684	1.988377
263.381430	1163.523025	18.549914	-0.049647	1.982746
263.552767	1155.588035	18.554919	-0.049674	1.977116
263.516347	1147.661933	18.559923	-0.049662	1.971454
263.471001	1139.741209	18.564928	-0.049648	1.965779
263.340879	1131.857134	18.569933	-0.049619	1.960104
263.245272	1123.947501	18.574938	-0.049596	1.954399
263.175936	1115.986927	18.579943	-0.049578	1.948642
263.139969	1108.066195	18.584947	-0.049566	1.942901
263.040390	1100.153334	18.589952	-0.049542	1.937142
262.951748	1092.252356	18.594957	-0.049521	1.931376
262.917502	1084.311363	18.599962	-0.049509	1.925569
263.031941	1076.405052	18.604967	-0.049525	1.919786
262.852603	1068.517861	18.609971	-0.049487	1.913967
262.673339	1060.594740	18.614976	-0.049448	1.908104
262.650513	1052.684398	18.619981	-0.049439	1.902250
262.639619	1044.770957	18.624986	-0.049432	1.896377
262.758598	1036.839876	18.629991	-0.049449	1.890487
262.624469	1028.948072	18.634995	-0.049418	1.884579
262.696804	1021.042789	18.640000	-0.049427	1.878666
262.613624	1013.145351	18.645005	-0.049406	1.872722
262.459657	1005.217870	18.650010	-0.049372	1.866729
262.377517	997.330109	18.655015	-0.049352	1.860755
262.416124	989.420477	18.660019	-0.049354	1.854759
262.164986	981.538361	18.665024	-0.049302	1.848730
262.315911	973.619433	18.670029	-0.049325	1.842701
262.111181	965.741418	18.675034	-0.049282	1.836642
262.149461	957.820540	18.680039	-0.049284	1.830558
262.004586	949.937554	18.685043	-0.049251	1.824461
262.096931	942.018653	18.690048	-0.049264	1.818344
262.199298	934.118303	18.695053	-0.049277	1.812223
261.733211	926.263762	18.700058	-0.049185	1.806048
261.910263	918.350295	18.705063	-0.049213	1.799883
261.953738	910.449467	18.710067	-0.049216	1.793691
261.842668	902.503797	18.715072	-0.049190	1.787423
261.848252	894.627907	18.720077	-0.049186	1.781202
261.697887	886.756551	18.725082	-0.049153	1.774945
261.625730	878.860909	18.730087	-0.049135	1.768655
261.596299	870.981443	18.735091	-0.049124	1.762361
261.485264	863.115809	18.740096	-0.049098	1.756045
261.560364	855.206418	18.745101	-0.049107	1.749695
261.185744	847.364129	18.750106	-0.049032	1.743319
261.132853	839.495820	18.755111	-0.049017	1.736939
261.319139	831.563897	18.760115	-0.049047	1.730514
261.199793	823.699839	18.765120	-0.049019	1.724082
261.222263	815.842323	18.770125	-0.049018	1.717649
261.101718	807.946661	18.775130	-0.048991	1.711143
261.187274	800.043891	18.780135	-0.049002	1.704632
261.139234	792.189247	18.785139	-0.048987	1.698118
261.045767	784.304089	18.790144	-0.048965	1.691549
260.974274	776.443512	18.795149	-0.048946	1.684977
260.786520	768.610836	18.800154	-0.048906	1.678387
260.710689	760.739464	18.805159	-0.048887	1.671753
260.798146	752.832489	18.810163	-0.048898	1.665085
260.653450	744.988242	18.815168	-0.048866	1.658412
260.639479	737.130339	18.820173	-0.048858	1.651719
260.450721	729.269964	18.825178	-0.048818	1.644971
260.407051	721.439146	18.830183	-0.048805	1.638242
260.320850	713.544109	18.835187	-0.048784	1.631423
260.281894	705.654037	18.840192	-0.048771	1.624586
260.330521	697.800687	18.845197	-0.048775	1.617765
260.186486	689.946993	18.850202	-0.048743	1.610888
260.099157	682.112315	18.855207	-0.048722	1.604005
260.044233	674.285916	18.860211	-0.048707	1.597105
259.975899	666.413417	18.865216	-0.048689	1.590132
259.885283	658.582018	18.870221	-0.048667	1.583162
259.834988	650.735341	18.875226	-0.048652	1.576153
259.881617	642.868975	18.880231	-0.048656	1.569110
259.649872	635.074830	18.885235	-0.048608	1.562058
259.496454	627.252408	18.890240	-0.048574	1.554961
259.667542	619.366261	18.895245	-0.048601	1.547821
259.458110	611.552000	18.900250	-0.048557	1.540657
259.574147	603.705601	18.905255	-0.048573	1.533479
259.526930	595.870200	18.910259	-0.048559	1.526253
259.418274	588.058322	18.915264	-0.048534	1.519005
259.502693	580.226026	18.920269	-0.048544	1.511732
259.254804	572.425958	18.925274	-0.048493	1.504404
259.419881	564.588035	18.930279	-0.048519	1.497067
259.245043	556.792511	18.935283	-0.048481	1.489682
259.063827	549.000523	18.940288	-0.048442	1.482262
258.930398	541.208151	18.945293	-0.048412	1.474812
258.828628	533.345214	18.950298	-0.048388	1.467262
258.868470	525.531679	18.955303	-0.048391	1.459742
258.733958	517.749129	18.960307	-0.048361	1.452186
258.688208	509.936382	18.965312	-0.048347	1.444575
258.791887	502.147608	18.970317	-0.048361	1.436972
258.731802	494.335987	18.975322	-0.048345	1.429278
258.857698	486.524645	18.980327	-0.048363	1.421574
258.795730	478.757005	18.985331	-0.048347	1.413841
258.554266	470.992722	18.990336	-0.048297	1.406038
258.631909	463.225029	18.995341	-0.048306	1.398242
258.344262	455.459279	19.000346	-0.048247	1.390342
258.325404	447.680095	19.005351	-0.048239	1.382430
258.337157	439.905248	19.010355	-0.048236	1.374481
257.993864	432.169730	19.015360	-0.048167	1.366465
258.029531	424.411343	19.020365	-0.048169	1.358444
257.993400	416.627284	19.025370	-0.048157	1.350336
258.104998	408.851380	19.030375	-0.048172	1.342214
257.980948	401.126352	19.035379	-0.048144	1.334054
257.810568	393.382227	19.040384	-0.048108	1.325815
258.051291	385.623397	19.045389	-0.048147	1.317583
257.658267	377.829715	19.050394	-0.048069	1.309147
257.517846	370.081253	19.055399	-0.048038	1.300751
257.664341	362.335318	19.060403	-0.048060	1.292356
257.608394	354.613919	19.065408	-0.048045	1.283896
257.631406	346.915753	19.070413	-0.048044	1.275420
257.364639	339.224794	19.075418	-0.047989	1.266840
257.273623	331.538005	19.080423	-0.047967	1.258240
257.329404	323.811304	19.085427	-0.047973	1.249564
257.353419	316.111009	19.090432	-0.047972	1.240851
257.290571	308.437474	19.095437	-0.047955	1.232090
257.170292	300.742823	19.100442	-0.047928	1.223231
256.856354	293.115888	19.105447	-0.047864	1.214348
256.986091	285.404675	19.110451	-0.047884	1.205388
257.028909	277.729059	19.115456	-0.047887	1.196387
256.849638	270.092365	19.120461	-0.047848	1.187318
256.736285	262.447330	19.125466	-0.047822	1.178182
256.776301	254.786161	19.130471	-0.047825	1.168988
256.685610	247.163705	19.135475	-0.047803	1.159740
256.381998	239.550564	19.140480	-0.047741	1.150385
256.430425	231.888897	19.145485	-0.047745	1.140967
256.255957	224.287397	19.150490	-0.047708	1.131499
256.358610	216.649552	19.155495	-0.047722	1.121964
256.303506	209.061586	19.160499	-0.047707	1.112377
256.352819	201.438828	19.165504	-0.047711	1.102685
256.125276	193.903701	19.170509	-0.047664	1.092958
255.732975	186.375134	19.175514	-0.047586	1.083116
255.848069	178.783282	19.180519	-0.047602	1.073215
255.757060	171.221496	19.185523	-0.047580	1.063214
255.560207	163.697753	19.190528	-0.047539	1.053145
255.566639	156.155887	19.195533	-0.047535	1.043002
255.645528	148.608522	19.200538	-0.047545	1.032768
255.535460	141.102997	19.205543	-0.047519	1.022445
255.500698	133.608596	19.210547	-0.047508	1.012050
255.272880	126.144640	19.215552	-0.047461	1.001543
255.211667	118.662932	19.220557	-0.047444	0.990940
255.060674	111.187909	19.225562	-0.047411	0.980210
254.911026	103.755529	19.230567	-0.047379	0.969423
254.962788	96.308909	19.235571	-0.047383	0.958545
254.780383	88.901522	19.240576	-0.047345	0.947540
254.928047	81.472638	19.245581	-0.047367	0.936460
254.856404	74.081501	19.250586	-0.047349	0.925247
254.535189	66.767078	19.255591	-0.047285	0.913947
254.225298	59.675399	19.260595	-0.047222	0.902856