Fri Mar 12 12:12:49 2021


Number of Points = 3626

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.620687	-0.101930	0.000000	-0.000059	0.720919
0.683498	-0.132684	0.005005	-0.000071	0.720881
0.577241	-0.115560	0.010010	-0.000051	0.720877
0.487514	-0.100230	0.015014	-0.000035	0.720876
0.844256	-0.162184	0.020019	-0.000101	0.720879
0.552682	-0.115153	0.025024	-0.000047	0.720870
0.744090	-0.144016	0.030029	-0.000083	0.720880
0.894599	-0.172378	0.035034	-0.000111	0.720877
0.713243	-0.140810	0.040038	-0.000077	0.720876
0.729103	-0.140713	0.045043	-0.000080	0.720881
0.634076	-0.127572	0.050048	-0.000062	0.720874
0.551193	-0.108225	0.055053	-0.000047	0.720883
0.456948	-0.095778	0.060058	-0.000029	0.720874
0.525851	-0.238930	0.065062	-0.000042	0.720617
0.474511	-0.266396	0.070067	-0.000032	0.720545
0.283668	-0.236626	0.075072	0.000003	0.720537
0.277734	-0.231657	0.080077	0.000004	0.720544
0.371830	-0.252273	0.085082	-0.000013	0.720537
0.345440	-0.247745	0.090086	-0.000008	0.720536
0.597739	-0.290349	0.095091	-0.000055	0.720541
0.607112	-0.419392	0.100096	-0.000057	0.720290
0.561806	-0.442645	0.105101	-0.000049	0.720229
0.615443	-0.455143	0.110106	-0.000059	0.720223
0.643522	-0.458968	0.115110	-0.000064	0.720225
0.643585	-0.456971	0.120115	-0.000064	0.720229
0.191614	-0.524794	0.125120	0.000020	0.719937
0.223443	-0.547390	0.130125	0.000014	0.719904
0.445112	-0.591316	0.135130	-0.000027	0.719895
0.370841	-0.576439	0.140134	-0.000013	0.719898
0.379508	-0.633921	0.145139	-0.000015	0.719788
0.411965	-0.737643	0.150144	-0.000021	0.719595
0.362544	-0.723787	0.155149	-0.000011	0.719605
0.227649	-0.701202	0.160154	0.000014	0.719602
0.291950	-0.803721	0.165158	0.000002	0.719423
0.621356	-0.937603	0.170163	-0.000060	0.719274
0.380935	-0.900140	0.175168	-0.000015	0.719264
0.358194	-0.912725	0.180173	-0.000011	0.719231
0.388483	-1.054953	0.185178	-0.000016	0.718961
0.283288	-1.036270	0.190182	0.000003	0.718961
0.324776	-1.041378	0.195187	-0.000004	0.718966
0.398090	-1.214469	0.200192	-0.000018	0.718650
0.556680	-1.242728	0.205197	-0.000047	0.718650
0.291407	-1.210125	0.210202	0.000002	0.718621
0.319235	-1.351641	0.215206	-0.000003	0.718351
0.502137	-1.380791	0.220211	-0.000037	0.718358
0.258945	-1.398592	0.225216	0.000008	0.718237
0.299102	-1.515485	0.230221	0.000001	0.718021
0.421893	-1.539383	0.235226	-0.000022	0.718017
0.330402	-1.641010	0.240230	-0.000005	0.717784
0.156652	-1.647553	0.245235	0.000027	0.717710
0.268782	-1.708290	0.250240	0.000006	0.717629
0.441861	-1.859463	0.255245	-0.000026	0.717391
0.335419	-1.843991	0.260250	-0.000006	0.717384
0.352567	-1.983448	0.265254	-0.000009	0.717115
0.327000	-1.990429	0.270259	-0.000004	0.717092
0.192805	-2.078655	0.275264	0.000021	0.716870
0.261107	-2.144829	0.280269	0.000008	0.716763
0.185238	-2.201086	0.285274	0.000022	0.716625
0.075121	-2.270072	0.290278	0.000043	0.716450
0.215345	-2.340277	0.295283	0.000017	0.716360
0.112134	-2.437452	0.300288	0.000036	0.716131
-0.156305	-2.414391	0.305293	0.000086	0.716082
-0.255378	-2.498157	0.310298	0.000104	0.715881
-0.060539	-2.558165	0.315302	0.000068	0.715831
-0.115909	-2.689959	0.320307	0.000078	0.715551
-0.498205	-2.644624	0.325312	0.000150	0.715505
-2.224220	-2.474089	0.330317	0.000471	0.715234
-4.209088	-2.121883	0.335322	0.000840	0.715231
-4.696519	-2.036006	0.340326	0.000931	0.715229
-3.663257	-2.345241	0.345331	0.000739	0.714981
-5.097098	-2.128794	0.350336	0.001006	0.714904
-5.303624	-2.088082	0.355341	0.001044	0.714912
-4.573940	-2.221078	0.360346	0.000908	0.714906
-5.309213	-2.220497	0.365350	0.001045	0.714647
-5.907397	-2.131201	0.370355	0.001156	0.714613
-5.876867	-2.141882	0.375360	0.001151	0.714602
-5.601210	-2.187741	0.380365	0.001099	0.714609
-6.088267	-2.157393	0.385370	0.001190	0.714497
-7.488402	-2.021147	0.390374	0.001451	0.714272
-6.466650	-2.199815	0.395379	0.001260	0.714279
-6.841529	-2.138305	0.400384	0.001330	0.714268
-7.057442	-2.095254	0.405389	0.001370	0.714277
-6.714063	-2.163438	0.410394	0.001306	0.714263
-7.549145	-2.165762	0.415398	0.001462	0.713963
-7.776210	-2.122297	0.420403	0.001504	0.713969
-8.108343	-2.066553	0.425408	0.001566	0.713962
-7.452866	-2.179931	0.430413	0.001444	0.713969
-7.380934	-2.195038	0.435418	0.001431	0.713965
-8.324337	-2.106300	0.440422	0.001606	0.713807
-8.542283	-2.144870	0.445427	0.001647	0.713653
-8.270270	-2.197547	0.450432	0.001596	0.713645
-8.755427	-2.108295	0.455437	0.001686	0.713650
-8.834120	-2.095936	0.460442	0.001701	0.713647
-8.502862	-2.155479	0.465446	0.001639	0.713646
-8.519861	-2.231952	0.470451	0.001643	0.713488
-9.970637	-2.041571	0.475456	0.001913	0.713353
-9.446986	-2.133314	0.480461	0.001815	0.713356
-9.317652	-2.157273	0.485466	0.001791	0.713354
-10.046059	-2.029233	0.490470	0.001927	0.713351
-9.307930	-2.155539	0.495475	0.001789	0.713361
-9.543820	-2.142915	0.500480	0.001833	0.713302
-10.666019	-2.083779	0.505485	0.002042	0.713022
-10.490196	-2.116884	0.510490	0.002009	0.713019
-10.757290	-2.071191	0.515494	0.002059	0.713015
-10.485728	-2.113745	0.520499	0.002008	0.713027
-10.515874	-2.114035	0.525504	0.002014	0.713015
-10.484380	-2.115777	0.530509	0.002008	0.713023
-10.166800	-2.237125	0.535514	0.001949	0.712894
-11.785630	-2.045232	0.540518	0.002250	0.712702
-11.213647	-2.144651	0.545523	0.002144	0.712707
-11.417630	-2.109848	0.550528	0.002182	0.712704
-11.577529	-2.078391	0.555533	0.002212	0.712710
-11.410424	-2.109669	0.560538	0.002180	0.712707
-11.499004	-2.097113	0.565542	0.002197	0.712701
-11.272666	-2.204683	0.570547	0.002155	0.712567
-12.631172	-2.059004	0.575552	0.002408	0.712375
-12.188577	-2.132511	0.580557	0.002325	0.712386
-12.054417	-2.157057	0.585562	0.002300	0.712384
-12.585868	-2.064530	0.590566	0.002399	0.712380
-12.169945	-2.133128	0.595571	0.002322	0.712391
-12.116711	-2.148504	0.600576	0.002312	0.712379
-12.354667	-2.202382	0.605581	0.002356	0.712188
-13.482910	-2.049930	0.610586	0.002566	0.712091
-13.330579	-2.081591	0.615590	0.002538	0.712082
-12.683221	-2.191941	0.620595	0.002417	0.712092
-13.365354	-2.075460	0.625600	0.002544	0.712082
-13.137559	-2.113792	0.630605	0.002502	0.712086
-12.941166	-2.148251	0.635610	0.002465	0.712087
-13.565414	-2.172017	0.640614	0.002582	0.711818
-14.237320	-2.079709	0.645619	0.002707	0.711764
-14.142485	-2.101123	0.650624	0.002689	0.711755
-13.866759	-2.148036	0.655629	0.002638	0.711759
-14.367449	-2.059615	0.660634	0.002731	0.711758
-14.186650	-2.094076	0.665638	0.002697	0.711753
-13.636249	-2.187506	0.670643	0.002595	0.711762
-14.562385	-2.137844	0.675648	0.002767	0.711532
-15.451055	-2.019066	0.680653	0.002932	0.711454
-14.742785	-2.145288	0.685658	0.002801	0.711454
-15.083236	-2.086866	0.690662	0.002864	0.711449
-15.060229	-2.087926	0.695667	0.002860	0.711455
-15.078985	-2.089293	0.700672	0.002863	0.711446
-15.022553	-2.094745	0.705677	0.002853	0.711455
-15.260059	-2.095673	0.710682	0.002897	0.711369
-16.079377	-2.067866	0.715686	0.003049	0.711133
-15.433980	-2.180307	0.720691	0.002929	0.711138
-16.043566	-2.078811	0.725696	0.003043	0.711124
-15.805222	-2.116369	0.730701	0.002998	0.711134
-15.576315	-2.156938	0.735706	0.002956	0.711134
-16.061667	-2.073826	0.740710	0.003046	0.711127
-16.162938	-2.087238	0.745715	0.003065	0.711065
-16.641420	-2.104944	0.750720	0.003154	0.710859
-16.474462	-2.129900	0.755725	0.003123	0.710869
-16.695312	-2.091770	0.760730	0.003164	0.710866
-16.638409	-2.105403	0.765734	0.003153	0.710859
-16.304245	-2.158826	0.770739	0.003091	0.710872
-16.588736	-2.113421	0.775744	0.003144	0.710861
-16.760065	-2.189387	0.780749	0.003176	0.710649
-17.288475	-2.157571	0.785754	0.003274	0.710524
-17.372882	-2.143323	0.790758	0.003290	0.710523
-17.419252	-2.130306	0.795763	0.003299	0.710532
-17.691941	-2.085984	0.800768	0.003349	0.710524
-17.254225	-2.160796	0.805773	0.003268	0.710530
-17.566900	-2.112397	0.810778	0.003326	0.710515
-18.576322	-2.087624	0.815782	0.003514	0.710205
-18.227505	-2.144214	0.820787	0.003449	0.710217
-18.577631	-2.087144	0.825792	0.003514	0.710206
-18.562338	-2.086757	0.830797	0.003511	0.710212
-18.404444	-2.111862	0.835802	0.003482	0.710218
-18.537632	-2.092241	0.840806	0.003507	0.710210
-18.517598	-2.093325	0.845811	0.003503	0.710215
-18.612066	-2.181793	0.850816	0.003521	0.710005
-19.528261	-2.075767	0.855821	0.003691	0.709890
-19.137422	-2.145512	0.860826	0.003618	0.709890
-19.578927	-2.070981	0.865830	0.003701	0.709882
-19.292498	-2.117277	0.870835	0.003647	0.709891
-19.365690	-2.108541	0.875840	0.003661	0.709883
-19.640418	-2.059672	0.880845	0.003712	0.709883
-19.604202	-2.126920	0.885850	0.003705	0.709761
-20.663432	-2.026873	0.890854	0.003902	0.709584
-20.175631	-2.109957	0.895859	0.003812	0.709591
-20.663545	-2.025630	0.900864	0.003902	0.709586
-20.619165	-2.032733	0.905869	0.003894	0.709588
-20.418552	-2.068968	0.910874	0.003857	0.709587
-20.544282	-2.049500	0.915878	0.003880	0.709581
-20.094118	-2.123497	0.920883	0.003796	0.709594
-20.521520	-2.195443	0.925888	0.003876	0.709297
-21.608436	-2.021170	0.930893	0.004078	0.709258
-21.232327	-2.086303	0.935898	0.004008	0.709262
-20.883479	-2.152700	0.940902	0.003943	0.709254
-21.219702	-2.086707	0.945907	0.004006	0.709266
-21.377140	-2.063342	0.950912	0.004035	0.709257
-21.064129	-2.118984	0.955917	0.003977	0.709257
-21.678023	-2.138045	0.960922	0.004091	0.709000
-22.503120	-2.019856	0.965926	0.004245	0.708942
-22.196828	-2.067363	0.970931	0.004188	0.708956
-22.276739	-2.056955	0.975936	0.004203	0.708949
-22.486432	-2.017802	0.980941	0.004242	0.708952
-22.179980	-2.072862	0.985946	0.004185	0.708951
-22.104137	-2.090758	0.990950	0.004170	0.708943
-22.315169	-2.089299	0.995955	0.004210	0.708870
-23.371430	-2.022698	1.000960	0.004406	0.708627
-22.834896	-2.117441	1.005965	0.004306	0.708628
-23.097798	-2.068844	1.010970	0.004355	0.708632
-23.059932	-2.077749	1.015974	0.004348	0.708628
-22.751999	-2.128281	1.020979	0.004291	0.708636
-23.059842	-2.076701	1.025984	0.004348	0.708630
-23.369034	-2.027920	1.030989	0.004406	0.708617
-23.563832	-2.128599	1.035994	0.004442	0.708346
-23.924010	-2.067494	1.040998	0.004509	0.708340
-23.913285	-2.065251	1.046003	0.004507	0.708348
-23.773156	-2.094057	1.051008	0.004481	0.708341
-23.960726	-2.061146	1.056013	0.004516	0.708340
-23.811512	-2.084755	1.061018	0.004488	0.708346
-24.294593	-2.002874	1.066022	0.004578	0.708337
-24.497167	-2.125627	1.071027	0.004616	0.708019
-24.703092	-2.097151	1.076032	0.004654	0.708002
-25.137075	-2.018061	1.081037	0.004735	0.708006
-24.734304	-2.087176	1.086042	0.004660	0.708011
-24.932074	-2.057390	1.091046	0.004697	0.708000
-25.034406	-2.035310	1.096051	0.004716	0.708008
-24.933993	-2.056724	1.101056	0.004697	0.708001
-25.018926	-2.152616	1.106061	0.004713	0.707778
-25.844592	-2.046714	1.111066	0.004867	0.707696
-26.080201	-2.008546	1.116070	0.004910	0.707688
-25.411127	-2.122990	1.121075	0.004786	0.707698
-25.784492	-2.061085	1.126080	0.004855	0.707688
-25.788848	-2.058532	1.131085	0.004856	0.707692
-25.702437	-2.071184	1.136090	0.004840	0.707698
-25.910598	-2.135763	1.141094	0.004879	0.707494
-26.834254	-2.030229	1.146099	0.005051	0.707375
-26.855646	-2.032458	1.151104	0.005055	0.707363
-26.643048	-2.067371	1.156109	0.005015	0.707369
-26.868906	-2.026270	1.161114	0.005057	0.707371
-27.208815	-1.968263	1.166118	0.005120	0.707365
-26.812784	-2.033733	1.171123	0.005047	0.707376
-26.695426	-2.060227	1.176128	0.005025	0.707365
-27.351773	-2.088763	1.181133	0.005147	0.707073
-27.604465	-2.043929	1.186138	0.005194	0.707072
-27.766193	-2.017486	1.191142	0.005224	0.707067
-27.337454	-2.091239	1.196147	0.005144	0.707073
-27.784836	-2.011390	1.201152	0.005228	0.707073
-27.534824	-2.057290	1.206157	0.005181	0.707070
-27.301926	-2.095862	1.211162	0.005138	0.707076
-28.506783	-2.046381	1.216166	0.005362	0.706744
-28.735088	-2.003872	1.221171	0.005404	0.706748
-28.567695	-2.037065	1.226176	0.005373	0.706741
-28.515489	-2.046695	1.231181	0.005364	0.706741
-28.550400	-2.036638	1.236186	0.005370	0.706748
-28.492543	-2.052560	1.241190	0.005359	0.706737
-28.287697	-2.084308	1.246195	0.005321	0.706747
-28.647742	-2.106089	1.251200	0.005388	0.706574
-29.883188	-1.956615	1.256205	0.005618	0.706432
-28.984216	-2.113419	1.261210	0.005451	0.706439
-29.638667	-2.000657	1.266214	0.005573	0.706431
-29.742394	-1.977441	1.271219	0.005592	0.706441
-29.357118	-2.049317	1.276224	0.005520	0.706434
-29.493016	-2.024523	1.281229	0.005545	0.706436
-29.647042	-2.021627	1.286234	0.005574	0.706386
-30.346338	-2.032272	1.291238	0.005704	0.706114
-29.861827	-2.114190	1.296243	0.005614	0.706123
-30.741976	-1.959637	1.301248	0.005778	0.706119
-30.558812	-1.992495	1.306253	0.005744	0.706118
-29.659572	-2.150711	1.311258	0.005576	0.706122
-30.543534	-1.996837	1.316262	0.005741	0.706115
-30.382041	-2.037673	1.321267	0.005711	0.706091
-30.817059	-2.077050	1.326272	0.005792	0.705856
-31.017748	-2.044082	1.331277	0.005829	0.705850
-31.100970	-2.024215	1.336282	0.005845	0.705860
-31.178482	-2.014447	1.341286	0.005859	0.705852
-30.675764	-2.099730	1.346291	0.005766	0.705861
-31.277300	-1.994684	1.351296	0.005877	0.705856
-31.313987	-2.058199	1.356301	0.005884	0.705716
-31.727366	-2.079723	1.361306	0.005961	0.705524
-31.809206	-2.070229	1.366310	0.005976	0.705514
-31.907891	-2.047568	1.371315	0.005995	0.705524
-31.944443	-2.044944	1.376320	0.006002	0.705516
-31.735845	-2.082027	1.381325	0.005963	0.705516
-32.124405	-2.009049	1.386330	0.006035	0.705524
-32.251196	-2.098232	1.391334	0.006059	0.705299
-32.589338	-2.082011	1.396339	0.006122	0.705210
-32.911648	-2.028831	1.401344	0.006182	0.705202
-33.292788	-1.960044	1.406349	0.006253	0.705203
-32.856468	-2.034701	1.411354	0.006171	0.705210
-32.930360	-2.026853	1.416358	0.006185	0.705199
-33.138246	-1.985696	1.421363	0.006224	0.705207
-32.785344	-2.122202	1.426368	0.006158	0.705059
-33.671590	-2.054796	1.431373	0.006323	0.704877
-33.227712	-2.130260	1.436378	0.006240	0.704884
-33.759642	-2.041411	1.441382	0.006339	0.704872
-33.514700	-2.079473	1.446387	0.006294	0.704884
-33.645543	-2.058136	1.451392	0.006318	0.704880
-34.121992	-1.974683	1.456397	0.006407	0.704877
-33.962137	-2.123846	1.461402	0.006377	0.704634
-34.700235	-2.019853	1.466406	0.006514	0.704578
-34.825657	-1.993090	1.471411	0.006538	0.704587
-34.511771	-2.052045	1.476416	0.006479	0.704581
-34.600555	-2.035300	1.481421	0.006496	0.704583
-34.544358	-2.043125	1.486426	0.006485	0.704587
-34.808284	-1.999533	1.491430	0.006535	0.704580
-34.747972	-2.125554	1.496435	0.006523	0.704348
-35.350281	-2.065578	1.501440	0.006635	0.704252
-35.606251	-2.020498	1.506445	0.006683	0.704251
-35.352542	-2.063575	1.511450	0.006636	0.704256
-35.463097	-2.048640	1.516454	0.006656	0.704246
-35.394514	-2.055654	1.521459	0.006644	0.704257
-35.278320	-2.080022	1.526464	0.006622	0.704249
-35.927256	-2.115376	1.531469	0.006743	0.703945
-36.102136	-2.082276	1.536474	0.006775	0.703949
-36.726565	-1.974869	1.541478	0.006892	0.703941
-36.227225	-2.060503	1.546483	0.006799	0.703948
-36.184184	-2.068809	1.551488	0.006791	0.703946
-36.485179	-2.016475	1.556493	0.006847	0.703944
-35.986692	-2.121189	1.561498	0.006754	0.703912
-36.712466	-2.133560	1.566502	0.006889	0.703626
-37.134251	-2.056013	1.571507	0.006967	0.703631
-37.359744	-2.016442	1.576512	0.007009	0.703629
-37.239464	-2.039370	1.581517	0.006987	0.703626
-37.192542	-2.044887	1.586522	0.006978	0.703632
-37.558930	-1.984643	1.591526	0.007046	0.703622
-37.051518	-2.085064	1.596531	0.006952	0.703602
-37.662923	-2.106893	1.601536	0.007066	0.703338
-38.465476	-1.966290	1.606541	0.007215	0.703333
-38.303317	-1.990576	1.611546	0.007185	0.703342
-37.939610	-2.061003	1.616550	0.007117	0.703331
-38.005371	-2.045773	1.621555	0.007129	0.703338
-38.217769	-2.009541	1.626560	0.007169	0.703335
-38.021783	-2.047281	1.631565	0.007133	0.703329
-38.213408	-2.165736	1.636570	0.007168	0.703021
-39.254228	-1.990606	1.641574	0.007362	0.703000
-39.312134	-1.977744	1.646579	0.007373	0.703005
-38.865985	-2.059238	1.651584	0.007290	0.703001
-39.124727	-2.012924	1.656589	0.007338	0.703002
-38.883869	-2.053796	1.661594	0.007293	0.703006
-38.717522	-2.090154	1.666598	0.007262	0.702992
-39.787653	-2.044630	1.671603	0.007461	0.702699
-40.065464	-2.002139	1.676608	0.007513	0.702685
-39.913234	-2.030222	1.681613	0.007485	0.702683
-39.310995	-2.134372	1.686618	0.007372	0.702689
-40.087829	-1.999891	1.691622	0.007517	0.702681
-39.891863	-2.032103	1.696627	0.007481	0.702687
-39.344379	-2.132129	1.701632	0.007379	0.702682
-40.576894	-2.070514	1.706637	0.007608	0.702362
-40.698961	-2.044477	1.711642	0.007631	0.702371
-40.764131	-2.037966	1.716646	0.007643	0.702361
-40.427164	-2.094974	1.721651	0.007580	0.702367
-40.622743	-2.060539	1.726656	0.007617	0.702366
-40.713998	-2.047176	1.731661	0.007634	0.702360
-40.441019	-2.119606	1.736666	0.007583	0.702312
-41.821898	-1.996252	1.741670	0.007840	0.702064
-41.509652	-2.047928	1.746675	0.007782	0.702072
-41.240465	-2.095825	1.751680	0.007732	0.702072
-41.690415	-2.016919	1.756685	0.007815	0.702069
-41.409811	-2.063648	1.761690	0.007763	0.702076
-41.517828	-2.048762	1.766694	0.007783	0.702067
-41.483123	-2.100458	1.771699	0.007777	0.701975
-42.807442	-1.980410	1.776704	0.008023	0.701740
-42.494797	-2.036443	1.781709	0.007965	0.701740
-42.479574	-2.035660	1.786714	0.007962	0.701747
-42.552910	-2.027842	1.791718	0.007976	0.701736
-42.379131	-2.056259	1.796723	0.007943	0.701742
-42.424318	-2.049834	1.801728	0.007952	0.701738
-42.627393	-2.012634	1.806733	0.007990	0.701740
-42.905667	-2.108139	1.811738	0.008041	0.701447
-43.367775	-2.034271	1.816742	0.008127	0.701429
-43.480119	-2.012786	1.821747	0.008148	0.701432
-43.115010	-2.076787	1.826752	0.008080	0.701435
-43.501142	-2.011454	1.831757	0.008152	0.701428
-43.151751	-2.068450	1.836762	0.008087	0.701438
-43.201866	-2.084624	1.841766	0.008096	0.701388
-44.215468	-2.035210	1.846771	0.008285	0.701122
-43.967526	-2.081055	1.851776	0.008239	0.701118
-44.484448	-1.991163	1.856781	0.008335	0.701114
-44.430255	-1.995946	1.861786	0.008325	0.701124
-44.511736	-1.985900	1.866790	0.008340	0.701115
-44.054857	-2.063338	1.871795	0.008255	0.701123
-44.197425	-2.040510	1.876800	0.008282	0.701118
-44.770158	-2.049241	1.881805	0.008388	0.700893
-44.942033	-2.027195	1.886810	0.008420	0.700876
-45.304223	-1.966472	1.891814	0.008488	0.700868
-45.264831	-1.969928	1.896819	0.008480	0.700875
-45.048742	-2.011133	1.901824	0.008440	0.700870
-45.131791	-1.996683	1.906829	0.008456	0.700869
-45.227299	-1.974465	1.911834	0.008473	0.700880
-45.372384	-2.078360	1.916838	0.008500	0.700617
-45.870525	-2.030586	1.921843	0.008593	0.700533
-45.761014	-2.050398	1.926848	0.008573	0.700533
-45.968628	-2.015775	1.931853	0.008611	0.700528
-45.595810	-2.077152	1.936858	0.008542	0.700538
-45.908579	-2.023507	1.941862	0.008600	0.700534
-46.092096	-2.020862	1.946867	0.008634	0.700473
-46.508687	-2.070719	1.951872	0.008712	0.700221
-46.670582	-2.046440	1.956877	0.008742	0.700212
-47.080795	-1.968411	1.961882	0.008818	0.700222
-46.995155	-1.989046	1.966886	0.008802	0.700211
-46.589937	-2.057629	1.971891	0.008727	0.700219
-46.616744	-2.052631	1.976896	0.008732	0.700219
-46.881528	-2.057797	1.981901	0.008781	0.700113
-47.577051	-2.038801	1.986906	0.008911	0.699900
-47.528596	-2.052879	1.991910	0.008902	0.699889
-47.861951	-1.989558	1.996915	0.008964	0.699897
-47.186272	-2.112157	2.001920	0.008838	0.699892
-47.691830	-2.020367	2.011917	0.008932	0.699896
-48.107947	-2.064249	2.021914	0.009009	0.699656
-48.460168	-2.030219	2.031910	0.009075	0.699598
-48.587053	-2.008464	2.041907	0.009099	0.699596
-48.439898	-2.036004	2.051904	0.009071	0.699594
-48.506148	-2.021675	2.061901	0.009083	0.699599
-47.990939	-2.113353	2.071898	0.008988	0.699599
-48.097884	-2.006482	2.081894	0.009007	0.699777
-47.716641	-2.017579	2.091891	0.008936	0.699893
-47.732309	-2.016622	2.101888	0.008939	0.699889
-47.641785	-2.032137	2.111885	0.008922	0.699891
-47.478129	-2.060117	2.121882	0.008892	0.699893
-47.578074	-2.043822	2.131878	0.008911	0.699890
-47.524944	-2.053708	2.141875	0.008901	0.699889
-47.840587	-1.988740	2.151872	0.008959	0.699907
-46.957280	-1.997666	2.161869	0.008795	0.700208
-46.761549	-2.031249	2.171866	0.008758	0.700211
-46.717140	-2.037693	2.181862	0.008750	0.700214
-46.755994	-2.031715	2.191859	0.008757	0.700212
-46.418524	-2.020745	2.201856	0.008694	0.700357
-45.757004	-2.053323	2.211853	0.008571	0.700530
-45.906594	-2.027405	2.221850	0.008599	0.700528
-45.897517	-2.028704	2.231846	0.008597	0.700529
-45.738850	-2.015927	2.241843	0.008568	0.700612
-45.012810	-2.021060	2.251840	0.008433	0.700864
-44.846508	-2.049894	2.261837	0.008402	0.700866
-44.689761	-2.076599	2.271834	0.008372	0.700869
-44.902246	-1.999159	2.281830	0.008412	0.700949
-43.978976	-2.082692	2.291827	0.008240	0.701113
-44.381532	-2.010084	2.301824	0.008315	0.701115
-44.402302	-2.005520	2.311821	0.008319	0.701117
-43.397440	-2.052670	2.321818	0.008132	0.701384
-43.555474	-2.001355	2.331814	0.008161	0.701431
-43.292528	-2.048655	2.341811	0.008112	0.701430
-43.308858	-1.994347	2.351808	0.008115	0.701534
-42.326803	-2.067507	2.361805	0.007932	0.701741
-42.426712	-2.048599	2.371802	0.007951	0.701743
-42.485081	-2.038410	2.381798	0.007962	0.701743
-41.677075	-2.051254	2.391795	0.007811	0.702008
-41.685258	-2.019297	2.401792	0.007813	0.702070
-41.569130	-2.040919	2.411789	0.007791	0.702068
-41.492828	-2.009958	2.421786	0.007777	0.702158
-40.906716	-2.011218	2.431782	0.007667	0.702367
-40.795962	-2.032964	2.441779	0.007647	0.702363
-41.039820	-1.986339	2.451776	0.007692	0.702370
-40.045732	-2.005704	2.461773	0.007507	0.702689
-39.901946	-2.031986	2.471770	0.007480	0.702688
-39.926265	-2.027793	2.481766	0.007485	0.702687
-39.605205	-1.987202	2.491763	0.007425	0.702885
-39.292846	-1.987479	2.501760	0.007367	0.702997
-39.001290	-2.039567	2.511757	0.007312	0.702997
-39.219887	-1.948920	2.521754	0.007353	0.703101
-38.067482	-2.039770	2.531750	0.007139	0.703333
-38.150237	-2.025777	2.541747	0.007154	0.703331
-38.208853	-2.014733	2.551744	0.007165	0.703332
-37.555622	-2.029281	2.561741	0.007043	0.703538
-37.439981	-2.005505	2.571738	0.007022	0.703628
-37.345973	-2.023300	2.581734	0.007004	0.703626
-37.413675	-1.963344	2.591731	0.007017	0.703723
-36.502460	-2.016580	2.601728	0.006847	0.703943
-36.397146	-2.032553	2.611725	0.006827	0.703949
-36.655375	-1.987045	2.621722	0.006875	0.703948
-35.854100	-1.987963	2.631718	0.006726	0.704234
-35.709490	-2.004158	2.641715	0.006699	0.704253
-35.573481	-2.029750	2.651712	0.006674	0.704251
-35.132246	-2.038966	2.661709	0.006592	0.704391
-34.628507	-2.032123	2.671706	0.006498	0.704585
-34.532210	-2.050171	2.681702	0.006480	0.704584
-34.996012	-1.968054	2.691699	0.006566	0.704583
-34.043901	-2.006277	2.701696	0.006389	0.704848
-33.911686	-2.011211	2.711693	0.006364	0.704885
-33.995091	-1.997105	2.721690	0.006380	0.704884
-33.567873	-1.991218	2.731686	0.006300	0.705049
-33.037583	-2.008304	2.741683	0.006201	0.705205
-33.087584	-1.999184	2.751680	0.006211	0.705206
-32.941470	-2.017960	2.761677	0.006183	0.705220
-32.132999	-2.012928	2.771674	0.006033	0.705520
-31.880871	-2.057046	2.781670	0.005986	0.705522
-32.287811	-1.985615	2.791667	0.006062	0.705520
-31.889312	-1.993679	2.801664	0.005987	0.705647
-30.936376	-2.057670	2.811661	0.005810	0.705860
-31.190227	-2.012405	2.821658	0.005857	0.705860
-31.108410	-2.028454	2.831654	0.005842	0.705857
-30.849605	-1.966418	2.841651	0.005794	0.706075
-30.399212	-2.025042	2.851648	0.005710	0.706118
-30.526988	-2.001707	2.861645	0.005734	0.706119
-30.268917	-1.961234	2.871642	0.005685	0.706293
-29.461924	-2.033327	2.881638	0.005535	0.706437
-29.932113	-1.951445	2.891635	0.005623	0.706434
-29.390141	-2.007243	2.901632	0.005522	0.706516
-28.819251	-1.995010	2.911629	0.005415	0.706745
-28.778648	-2.002624	2.921626	0.005408	0.706744
-28.689809	-2.018292	2.931622	0.005391	0.706744
-28.109933	-1.974534	2.941619	0.005283	0.707040
-27.659609	-2.037897	2.951616	0.005199	0.707074
-27.882775	-1.997404	2.961613	0.005241	0.707075
-27.738099	-1.965834	2.971610	0.005214	0.707191
-26.969722	-2.012052	2.981606	0.005071	0.707373
-27.130833	-1.984646	2.991603	0.005101	0.707370
-26.922341	-2.021562	3.001600	0.005062	0.707371
-26.324950	-1.966408	3.011597	0.004951	0.707695
-26.042983	-2.014394	3.021594	0.004898	0.707700
-25.885212	-2.044607	3.031590	0.004869	0.707696
-25.976657	-1.965869	3.041587	0.004886	0.707821
-25.207547	-2.009397	3.051584	0.004743	0.708008
-25.220424	-2.005842	3.061581	0.004745	0.708011
-25.205869	-2.008658	3.071578	0.004742	0.708011
-24.486103	-1.970321	3.081574	0.004608	0.708345
-24.110492	-2.036124	3.091571	0.004538	0.708347
-24.099569	-2.038331	3.101568	0.004536	0.708347
-24.335122	-1.946566	3.111565	0.004580	0.708446
-23.340171	-2.029083	3.121562	0.004395	0.708636
-23.392836	-2.019489	3.131558	0.004404	0.708637
-23.543829	-1.994828	3.141555	0.004433	0.708632
-22.719892	-1.998827	3.151552	0.004279	0.708918
-22.898372	-1.949751	3.161549	0.004312	0.708953
-22.237479	-2.065380	3.171546	0.004189	0.708957
-22.553300	-1.943960	3.181542	0.004248	0.709088
-21.602307	-2.026512	3.191539	0.004071	0.709262
-21.649501	-2.019143	3.201536	0.004080	0.709260
-21.845436	-1.983976	3.211533	0.004116	0.709260
-20.818598	-2.005282	3.221530	0.003925	0.709584
-21.020264	-1.964523	3.231526	0.003962	0.709594
-20.800567	-2.003625	3.241523	0.003921	0.709594
-20.598083	-1.971978	3.251520	0.003884	0.709729
-19.898348	-2.016190	3.261517	0.003753	0.709890
-20.018648	-1.994699	3.271514	0.003776	0.709890
-20.281592	-1.927694	3.281510	0.003825	0.709931
-19.162823	-1.985944	3.291507	0.003616	0.710213
-19.119785	-1.993054	3.301504	0.003608	0.710214
-19.095187	-1.996564	3.311501	0.003604	0.710216
-18.553864	-1.986313	3.321498	0.003503	0.710429
-18.433925	-1.957399	3.331494	0.003481	0.710530
-18.169044	-2.005020	3.341491	0.003431	0.710529
-18.153543	-1.988675	3.351488	0.003428	0.710567
-17.253502	-1.996921	3.361485	0.003261	0.710871
-16.990687	-2.043351	3.371482	0.003212	0.710872
-17.423517	-1.967539	3.381478	0.003292	0.710869
-17.157555	-1.963047	3.391475	0.003243	0.710973
-16.524507	-1.993612	3.401472	0.003125	0.711137
-16.591352	-1.981766	3.411469	0.003137	0.711137
-16.630023	-1.951207	3.421466	0.003144	0.711184
-15.994170	-1.930295	3.431462	0.003026	0.711452
-15.627020	-1.995510	3.441459	0.002958	0.711453
-15.891717	-1.949035	3.451456	0.003007	0.711451
-15.018148	-1.963529	3.461453	0.002844	0.711733
-14.698102	-2.008433	3.471450	0.002785	0.711757
-14.911119	-1.970188	3.481446	0.002824	0.711758
-14.565048	-1.958925	3.491443	0.002760	0.711903
-13.900643	-1.985467	3.501440	0.002636	0.712086
-13.852433	-1.992201	3.511437	0.002627	0.712090
-13.929971	-1.977823	3.521434	0.002641	0.712091
-13.227034	-1.969932	3.531430	0.002510	0.712356
-12.899477	-2.012787	3.541427	0.002449	0.712387
-13.011498	-1.993874	3.551424	0.002470	0.712385
-12.947311	-1.954093	3.561421	0.002458	0.712487
-11.981150	-2.013239	3.571418	0.002278	0.712712
-11.887707	-2.030346	3.581414	0.002261	0.712712
-12.056503	-2.001906	3.591411	0.002292	0.712708
-11.641146	-1.979010	3.601408	0.002215	0.712901
-11.075697	-2.017074	3.611405	0.002110	0.713026
-11.253387	-1.985048	3.621402	0.002143	0.713027
-11.268040	-1.966127	3.631398	0.002145	0.713059
-10.350266	-1.978910	3.641395	0.001974	0.713359
-10.317752	-1.985044	3.651392	0.001968	0.713359
-10.061950	-2.029036	3.661389	0.001921	0.713362
-10.000739	-1.962792	3.671386	0.001909	0.713515
-8.539463	-2.153681	3.681382	0.001637	0.713654
-8.760194	-2.115874	3.691379	0.001678	0.713651
-8.848319	-2.099688	3.701376	0.001695	0.713652
-8.599353	-2.142736	3.711373	0.001648	0.713654
-8.191772	-2.074114	3.721370	0.001572	0.713935
-8.050387	-2.081673	3.731366	0.001546	0.713970
-7.990279	-2.093549	3.741363	0.001535	0.713968
-7.972073	-2.095246	3.751360	0.001531	0.713971
-7.045447	-2.109037	3.761357	0.001359	0.714272
-7.174943	-2.081389	3.771354	0.001383	0.714281
-7.087922	-2.098926	3.781350	0.001367	0.714277
-7.354791	-2.014383	3.791347	0.001416	0.714350
-6.191802	-2.092909	3.801344	0.001200	0.714606
-5.830018	-2.155579	3.811341	0.001132	0.714610
-6.174555	-2.095444	3.821338	0.001197	0.714607
-5.851370	-2.106438	3.831334	0.001136	0.714700
-5.374182	-2.088236	3.841331	0.001047	0.714905
-5.316543	-2.097468	3.851328	0.001037	0.714907
-5.291569	-2.101392	3.861325	0.001032	0.714908
-4.717988	-2.087448	3.871322	0.000925	0.715138
-4.262497	-2.121618	3.881318	0.000840	0.715231
-4.563545	-2.068644	3.891315	0.000896	0.715230
-4.253634	-2.113163	3.901312	0.000839	0.715251
-3.584860	-2.083283	3.911309	0.000714	0.715547
-3.297433	-2.135103	3.921306	0.000661	0.715546
-3.228733	-2.147605	3.931302	0.000648	0.715545
-3.511102	-2.044308	3.941299	0.000700	0.715650
-2.748567	-2.063499	3.951296	0.000558	0.715882
-2.509668	-2.103283	3.961293	0.000514	0.715887
-2.565441	-2.093768	3.971290	0.000524	0.715886
-2.182924	-2.052479	3.981286	0.000453	0.716103
-1.910900	-2.086090	3.991283	0.000402	0.716133
-1.897661	-2.086857	4.001280	0.000400	0.716136
-1.814376	-2.009864	4.011277	0.000384	0.716318
-1.952079	-1.917836	4.021274	0.000410	0.716452
-1.689087	-1.964670	4.031270	0.000361	0.716452
-1.361806	-1.877481	4.041267	0.000300	0.716740
-1.316617	-1.877502	4.051264	0.000291	0.716756
-1.155442	-1.833615	4.061261	0.000261	0.716899
-0.931134	-1.777888	4.071258	0.000219	0.717089
-1.148234	-1.714789	4.081254	0.000260	0.717137
-1.150649	-1.592010	4.091251	0.000260	0.717379
-1.314331	-1.513951	4.101248	0.000290	0.717476
-0.840754	-1.484990	4.111245	0.000202	0.717700
-0.828321	-1.407196	4.121242	0.000200	0.717858
-0.612731	-1.366597	4.131238	0.000160	0.718014
-0.737235	-1.214442	4.141235	0.000183	0.718271
-0.979936	-1.095456	4.151232	0.000228	0.718421
-0.678503	-1.037462	4.161229	0.000172	0.718641
-0.687311	-0.906830	4.171226	0.000173	0.718896
-0.611521	-0.822042	4.181222	0.000159	0.719090
-0.522864	-0.732187	4.191219	0.000142	0.719299
-0.458510	-0.592148	4.201216	0.000130	0.719597
-0.548679	-0.449869	4.211213	0.000147	0.719846
-0.482409	-0.332589	4.221210	0.000134	0.720101
-0.259922	-0.238162	4.231206	0.000093	0.720365
-0.193393	-0.112299	4.241203	0.000080	0.720636
-0.313420	0.056449	4.251200	0.000103	0.720926
0.000000	0.165964	4.261197	0.000044	0.721251
-0.196881	0.825020	4.266202	0.000080	0.722477
-0.131755	2.077260	4.271206	0.000067	0.724955
0.103596	3.885622	4.276211	0.000022	0.728566
0.277158	6.261313	4.281216	-0.000011	0.733237
0.624643	9.115299	4.286221	-0.000078	0.738856
0.682353	12.489950	4.291226	-0.000091	0.745326
1.242417	16.242635	4.296230	-0.000198	0.752622
1.485281	20.451802	4.301235	-0.000246	0.760594
1.711420	25.061727	4.306240	-0.000291	0.769218
2.172873	29.999754	4.311245	-0.000380	0.778419
2.635879	35.277290	4.316250	-0.000470	0.788125
2.897450	40.916570	4.321254	-0.000522	0.798292
3.258198	46.836725	4.326259	-0.000593	0.808855
3.671595	53.025320	4.331264	-0.000674	0.819762
4.209780	59.477180	4.336269	-0.000779	0.831013
4.489031	66.184440	4.341274	-0.000835	0.842466
4.922585	73.095249	4.346278	-0.000920	0.854148
5.274110	80.220862	4.351283	-0.000990	0.866001
5.832171	87.490824	4.356288	-0.001099	0.877986
6.570733	94.921689	4.361293	-0.001241	0.890116
6.885622	102.569644	4.366298	-0.001305	0.902306
7.072907	110.403374	4.371302	-0.001345	0.914588
7.411711	118.300462	4.376307	-0.001413	0.926844
8.367315	126.220988	4.381312	-0.001596	0.939138
11.117340	133.970831	4.386317	-0.002113	0.951486
11.660885	142.195886	4.391322	-0.002220	0.963806
12.067057	150.541535	4.396326	-0.002301	0.976112
13.223196	158.829711	4.401331	-0.002522	0.988368
13.940960	167.245842	4.406336	-0.002661	1.000547
14.998243	175.654816	4.411341	-0.002863	1.012652
16.036413	184.112853	4.416346	-0.003062	1.024676
16.977161	192.644829	4.421350	-0.003243	1.036639
17.586412	201.250516	4.426355	-0.003362	1.048486
18.406330	209.847009	4.431360	-0.003520	1.060237
19.284967	218.471097	4.436365	-0.003689	1.071909
20.036955	227.092420	4.441370	-0.003835	1.083422
20.803918	235.730549	4.446374	-0.003984	1.094839
21.846263	244.321480	4.451379	-0.004183	1.106138
22.637286	252.972786	4.456384	-0.004336	1.117343
23.363505	261.628524	4.461389	-0.004477	1.128429
23.869667	270.316218	4.466394	-0.004577	1.139399
24.430880	279.011077	4.471398	-0.004687	1.150285
24.855997	287.704572	4.476403	-0.004772	1.161039
26.039029	296.231198	4.481408	-0.004998	1.171648
26.914234	304.822757	4.486413	-0.005166	1.182176
27.859542	313.391769	4.491418	-0.005348	1.192598
28.496425	321.993808	4.496422	-0.005472	1.202907
29.197471	330.595124	4.501427	-0.005608	1.213139
29.946977	339.159192	4.506432	-0.005754	1.223252
30.326090	347.808633	4.511437	-0.005830	1.233308
30.825825	356.367027	4.516442	-0.005928	1.243201
31.748548	364.867395	4.521446	-0.006106	1.253032
32.353317	373.405292	4.526451	-0.006224	1.262767
32.840584	381.941509	4.531456	-0.006320	1.272404
33.694946	390.394052	4.536461	-0.006485	1.281944
33.980329	398.938176	4.541466	-0.006544	1.291408
34.853288	407.362818	4.546470	-0.006712	1.300781
35.527639	415.880716	4.551475	-0.006843	1.310151
36.005757	424.416449	4.556480	-0.006937	1.319438
36.622659	432.828441	4.561485	-0.007058	1.328553
37.201715	441.243548	4.566490	-0.007171	1.337602
37.950894	449.611129	4.571494	-0.007316	1.346570
38.628376	458.021016	4.576499	-0.007448	1.355509
39.109813	466.407697	4.581504	-0.007543	1.364332
40.027099	474.753819	4.586509	-0.007719	1.373131
40.354454	483.160042	4.591514	-0.007786	1.381835
41.022944	491.524006	4.596518	-0.007915	1.390499
41.770576	499.870454	4.601523	-0.008060	1.399104
42.493871	508.179691	4.606528	-0.008200	1.407615
42.884870	516.578954	4.611533	-0.008279	1.416110
43.570066	524.885433	4.616538	-0.008412	1.424509
44.157070	533.234210	4.621542	-0.008526	1.432885
44.656543	541.568109	4.626547	-0.008625	1.441184
45.306738	549.862611	4.631552	-0.008751	1.449420
45.784600	558.215940	4.636557	-0.008846	1.457639
46.361342	566.485930	4.641562	-0.008958	1.465747
47.272003	574.778808	4.646566	-0.009133	1.473885
47.725170	583.087463	4.651571	-0.009223	1.481921
48.178006	591.368734	4.656576	-0.009313	1.489888
48.659199	599.678150	4.661581	-0.009408	1.497843
48.942140	607.960277	4.666586	-0.009466	1.505699
49.526558	616.232116	4.671590	-0.009580	1.513551
49.951114	624.496473	4.676595	-0.009665	1.521332
50.473663	632.744503	4.681600	-0.009767	1.529072
51.039808	641.008658	4.686605	-0.009878	1.536794
51.422446	649.258290	4.691610	-0.009955	1.544437
51.715326	657.563865	4.696614	-0.010015	1.552080
52.306131	665.782847	4.701619	-0.010130	1.559650
52.668137	674.000763	4.706624	-0.010203	1.567149
53.026052	682.270475	4.711629	-0.010275	1.574659
53.525766	690.466978	4.716634	-0.010373	1.582087
54.414531	698.630896	4.721638	-0.010544	1.589507
55.506820	706.787950	4.726643	-0.010753	1.596916
55.922526	715.010483	4.731648	-0.010836	1.604252
56.582952	723.232818	4.736653	-0.010964	1.611588
56.875455	731.495283	4.741658	-0.011024	1.618875
57.432757	739.702632	4.746662	-0.011133	1.626118
57.894951	747.986574	4.751667	-0.011225	1.633381
58.213461	756.192395	4.756672	-0.011289	1.640525
58.759969	764.370078	4.761677	-0.011396	1.647645
59.419611	772.543157	4.766682	-0.011525	1.654746
60.166169	780.681692	4.771686	-0.011669	1.661799
60.445187	788.923284	4.776691	-0.011726	1.668845
60.531475	797.165614	4.781696	-0.011748	1.675837
61.086187	805.326197	4.786701	-0.011856	1.682794
61.503220	813.507578	4.791706	-0.011939	1.689720
62.031063	821.688487	4.796710	-0.012043	1.696633
62.925628	829.801170	4.801715	-0.012215	1.703509
63.678664	837.950682	4.806720	-0.012360	1.710369
64.281632	846.157358	4.811725	-0.012478	1.717228
64.824664	854.306597	4.816730	-0.012584	1.724006
65.180194	862.498671	4.821734	-0.012656	1.730767
65.684592	870.682792	4.826739	-0.012755	1.737515
65.782140	878.892052	4.831744	-0.012779	1.744205
66.475108	887.034813	4.836749	-0.012913	1.750891
67.021438	895.186614	4.841754	-0.013020	1.757541
67.643080	903.321942	4.846758	-0.013141	1.764161
68.082440	911.504392	4.851763	-0.013228	1.770771
68.560865	919.668896	4.856768	-0.013323	1.777347
68.939498	927.845433	4.861773	-0.013399	1.783896
69.058611	936.068625	4.866778	-0.013426	1.790426
69.743467	944.223386	4.871782	-0.013559	1.796947
70.292338	952.337663	4.876787	-0.013667	1.803396
70.707461	960.468904	4.881792	-0.013749	1.809819
71.315675	968.604645	4.886797	-0.013868	1.816246
71.772747	976.726408	4.891802	-0.013958	1.822621
72.218819	984.869890	4.896806	-0.014046	1.828990
72.729379	993.020749	4.901811	-0.014147	1.835349
73.383136	1001.108737	4.906816	-0.014274	1.841655
73.698365	1009.284362	4.911821	-0.014338	1.847966
73.828959	1017.481594	4.916826	-0.014368	1.854251
74.622549	1025.547261	4.921830	-0.014521	1.860492
75.112250	1033.693799	4.926835	-0.014617	1.866737
74.958974	1041.927629	4.931840	-0.014594	1.872953
75.391474	1050.043250	4.936845	-0.014680	1.879128
75.923355	1058.129895	4.941850	-0.014784	1.885271
76.385251	1066.252602	4.946854	-0.014875	1.891413
76.734202	1074.399009	4.951859	-0.014946	1.897540
76.953864	1082.526620	4.956864	-0.014992	1.903619
77.435269	1090.655736	4.961869	-0.015087	1.909709
77.859208	1098.777271	4.966874	-0.015171	1.915767
78.594266	1106.833194	4.971878	-0.015313	1.921792
78.982887	1114.972437	4.976883	-0.015391	1.927821
79.269901	1123.119778	4.981888	-0.015450	1.933826
79.693868	1131.244513	4.986893	-0.015534	1.939811
80.320807	1139.324316	4.991898	-0.015656	1.945767
80.654741	1147.487187	4.996902	-0.015724	1.951732
81.215381	1155.616752	5.001907	-0.015833	1.957680
81.637879	1163.695425	5.006912	-0.015917	1.963558
82.171869	1171.804390	5.011917	-0.016022	1.969452
82.200080	1179.973330	5.016922	-0.016032	1.975318
82.488640	1188.074031	5.021926	-0.016091	1.981145
82.653092	1196.198916	5.026931	-0.016127	1.986958
83.057197	1204.311681	5.031936	-0.016208	1.992772
83.509500	1212.411360	5.036941	-0.016297	1.998564
83.860831	1220.499064	5.041946	-0.016368	2.004320
84.068720	1228.612953	5.046950	-0.016412	2.010064
84.532965	1236.730773	5.051955	-0.016504	2.015820
85.067580	1244.786442	5.056960	-0.016609	2.021523
85.393511	1252.902362	5.061965	-0.016675	2.027231
85.409826	1261.086831	5.066970	-0.016683	2.032939
85.901624	1269.156474	5.071974	-0.016780	2.038599
86.459190	1277.215398	5.076979	-0.016889	2.044243
86.593061	1285.327803	5.081984	-0.016919	2.049866
87.065510	1293.427502	5.086989	-0.017013	2.055498
87.422766	1301.510290	5.091994	-0.017084	2.061091
87.716620	1309.612294	5.096998	-0.017144	2.066676
88.078614	1317.750292	5.102003	-0.017217	2.072278
88.482367	1325.813998	5.107008	-0.017298	2.077817
88.968166	1333.887157	5.112013	-0.017393	2.083357
89.411833	1341.969199	5.117018	-0.017481	2.088883
89.539684	1350.117237	5.122022	-0.017510	2.094409
90.073531	1358.186591	5.127027	-0.017615	2.099906
90.172194	1366.309170	5.132032	-0.017639	2.105382
90.512876	1374.441520	5.137037	-0.017707	2.110874
90.946930	1382.549400	5.142042	-0.017793	2.116345
91.501456	1390.571362	5.147046	-0.017902	2.121755
91.880724	1398.646982	5.152051	-0.017978	2.127171
91.972006	1406.773131	5.157056	-0.018000	2.132578
92.452280	1414.845506	5.162061	-0.018095	2.137973
92.719687	1422.926852	5.167066	-0.018150	2.143341
92.929458	1431.015592	5.172070	-0.018194	2.148694
93.563936	1439.104581	5.177075	-0.018318	2.154074
93.580988	1447.215266	5.182080	-0.018326	2.159397
93.886777	1455.296219	5.187085	-0.018388	2.164714
94.360705	1463.358976	5.192090	-0.018482	2.170022
94.728395	1471.449030	5.197094	-0.018556	2.175325
94.987317	1479.551946	5.202099	-0.018609	2.180613
95.206333	1487.630236	5.207104	-0.018655	2.185868
95.731906	1495.720748	5.212109	-0.018758	2.191147
95.929898	1503.840427	5.217114	-0.018801	2.196402
96.158257	1511.899153	5.222118	-0.018848	2.201608
96.372922	1519.979795	5.227123	-0.018894	2.206815
96.605522	1528.060082	5.232128	-0.018942	2.212010
97.006963	1536.127485	5.237133	-0.019022	2.217200
97.640546	1544.146675	5.242138	-0.019145	2.222368
97.765642	1552.243292	5.247142	-0.019174	2.227528
98.246215	1560.338807	5.252147	-0.019269	2.232707
98.482935	1568.422644	5.257152	-0.019318	2.237844
98.716619	1576.494484	5.262157	-0.019367	2.242962
99.069239	1584.571329	5.267162	-0.019438	2.248082
99.149038	1592.675510	5.272166	-0.019458	2.253183
99.754694	1600.730228	5.277171	-0.019576	2.258288
100.195482	1608.774065	5.282176	-0.019663	2.263360
100.272124	1616.908294	5.287181	-0.019683	2.268445
100.614763	1625.063394	5.292186	-0.019752	2.273555
100.619812	1633.128400	5.297190	-0.019758	2.278568
101.057651	1641.153938	5.302195	-0.019845	2.283583
101.089167	1649.232002	5.307200	-0.019856	2.288584
101.500252	1657.300306	5.312205	-0.019938	2.293601
101.944504	1665.335091	5.317210	-0.020026	2.298589
102.070347	1673.405442	5.322214	-0.020055	2.303561
102.540713	1681.456788	5.327219	-0.020148	2.308540
102.578451	1689.576152	5.332224	-0.020160	2.313513
102.674163	1697.660583	5.337229	-0.020183	2.318459
102.948779	1705.710754	5.342234	-0.020239	2.323389
103.130739	1713.769785	5.347238	-0.020279	2.328306
103.465940	1721.849584	5.352243	-0.020346	2.333237
103.588993	1729.918279	5.357248	-0.020374	2.338134
103.926642	1737.974077	5.362253	-0.020443	2.343030
104.253121	1746.032677	5.367258	-0.020509	2.347917
104.324471	1754.144389	5.372262	-0.020527	2.352805
104.746485	1762.202217	5.377267	-0.020611	2.357679
104.972989	1770.239004	5.382272	-0.020658	2.362514
105.275873	1778.302241	5.387277	-0.020720	2.367361
105.544824	1786.378407	5.392282	-0.020775	2.372203
106.011398	1794.412706	5.397286	-0.020868	2.377027
106.368543	1802.484375	5.402291	-0.020939	2.381853
106.403794	1810.556268	5.407296	-0.020951	2.386645
106.850462	1818.636088	5.412301	-0.021040	2.391464
107.078378	1826.716515	5.417306	-0.021087	2.396256
107.190746	1834.763508	5.422310	-0.021114	2.401010
107.355823	1842.844471	5.427315	-0.021150	2.405779
107.724481	1850.891897	5.432320	-0.021223	2.410535
107.939339	1858.984956	5.437325	-0.021269	2.415295
108.164096	1867.043677	5.442330	-0.021316	2.420027
108.441236	1875.080082	5.447334	-0.021373	2.424741
108.908215	1883.140999	5.452339	-0.021465	2.429475
108.957550	1891.302108	5.457344	-0.021479	2.434225
109.169883	1899.330660	5.462349	-0.021524	2.438901
109.486272	1907.358374	5.467354	-0.021588	2.443576
109.540604	1915.409100	5.472358	-0.021604	2.448236
109.825976	1923.484952	5.477363	-0.021662	2.452918
110.216560	1931.506765	5.482368	-0.021740	2.457569
110.674848	1939.528379	5.487373	-0.021831	2.462215
110.875271	1947.596963	5.492378	-0.021873	2.466861
111.292052	1955.643391	5.497382	-0.021956	2.471500
111.494806	1963.757149	5.502387	-0.021999	2.476154
111.646895	1971.801171	5.507392	-0.022033	2.480755
111.913658	1979.843694	5.512397	-0.022088	2.485356
112.013784	1987.930328	5.517402	-0.022112	2.489961
112.198748	1995.990180	5.522406	-0.022151	2.494548
112.460841	2004.038471	5.527411	-0.022205	2.499125
112.593541	2012.096013	5.532416	-0.022235	2.503691
112.950958	2020.157107	5.537421	-0.022307	2.508266
113.133548	2028.260925	5.542426	-0.022347	2.512844
113.496060	2036.299560	5.547430	-0.022419	2.517390
113.957104	2044.312202	5.552435	-0.022510	2.521920
114.245305	2052.346913	5.557440	-0.022569	2.526442
114.448639	2060.403711	5.562445	-0.022612	2.530963
114.754902	2068.498845	5.567450	-0.022675	2.535503
114.988252	2076.520136	5.572454	-0.022723	2.539990
115.205650	2084.578017	5.577459	-0.022769	2.544487
115.394233	2092.650022	5.582464	-0.022810	2.548983
115.747275	2100.718626	5.587469	-0.022881	2.553480
115.875490	2108.777656	5.592474	-0.022910	2.557948
116.198089	2116.797412	5.597478	-0.022975	2.562400
116.500635	2124.861909	5.602483	-0.023037	2.566867
116.684939	2132.910152	5.607488	-0.023076	2.571310
116.886592	2140.997831	5.612493	-0.023119	2.575768
117.160964	2149.039237	5.617498	-0.023175	2.580197
117.377542	2157.069366	5.622502	-0.023221	2.584609
117.738594	2165.150977	5.627507	-0.023293	2.589052
118.021192	2173.357017	5.632512	-0.023351	2.593549
118.233279	2181.390402	5.637517	-0.023396	2.597939
118.545771	2189.397690	5.642522	-0.023460	2.602315
118.696370	2197.397384	5.647526	-0.023493	2.606668
119.244591	2205.431995	5.652531	-0.023600	2.611060
119.179897	2213.497696	5.657536	-0.023593	2.615419
119.439971	2221.522089	5.662541	-0.023647	2.619771
119.894051	2229.552190	5.667546	-0.023737	2.624132
119.925047	2237.602672	5.672550	-0.023748	2.628468
120.301577	2245.678472	5.677555	-0.023823	2.632834
120.418514	2253.714883	5.682560	-0.023850	2.637153
120.826507	2261.731070	5.687565	-0.023932	2.641475
121.083909	2269.762775	5.692570	-0.023985	2.645787
121.247241	2277.803774	5.697574	-0.024020	2.650091
121.743128	2285.857673	5.702579	-0.024118	2.654417
121.659545	2293.930982	5.707584	-0.024108	2.658708
121.790695	2301.982262	5.712589	-0.024137	2.662995
122.279354	2309.994196	5.717594	-0.024234	2.667276
122.435060	2318.088129	5.722598	-0.024268	2.671573
122.593206	2326.188396	5.727603	-0.024303	2.675867
122.924738	2334.171255	5.732608	-0.024370	2.680102
123.405978	2342.166006	5.737613	-0.024464	2.684347
123.745800	2350.238888	5.742618	-0.024533	2.688617
123.910292	2358.285316	5.747622	-0.024569	2.692855
124.162810	2366.372632	5.752627	-0.024621	2.697113
124.123750	2374.427428	5.757632	-0.024619	2.701330
124.236164	2382.468834	5.762637	-0.024645	2.705542
124.812112	2390.489401	5.767642	-0.024758	2.709766
125.226147	2398.534416	5.772646	-0.024840	2.713985
125.326451	2406.607488	5.777651	-0.024864	2.718193
125.699757	2414.612461	5.782656	-0.024939	2.722377
126.164657	2422.631100	5.787661	-0.025031	2.726566
126.314453	2430.710680	5.792666	-0.025064	2.730761
126.517440	2438.772907	5.797670	-0.025107	2.734944
126.904171	2446.804645	5.802675	-0.025184	2.739116
127.146129	2454.825400	5.807680	-0.025234	2.743267
127.259917	2462.904539	5.812685	-0.025261	2.747434
127.443298	2471.003000	5.817690	-0.025300	2.751609
127.664055	2479.089387	5.822694	-0.025347	2.755773
128.092509	2487.075336	5.827699	-0.025432	2.759892
128.227808	2495.082846	5.832704	-0.025462	2.763999
128.577490	2503.115743	5.837709	-0.025533	2.768125
128.818705	2511.180256	5.842714	-0.025583	2.772254
128.998866	2519.237087	5.847718	-0.025621	2.776370
129.635569	2527.231259	5.852723	-0.025745	2.780475
129.797016	2535.256643	5.857728	-0.025781	2.784561
129.860926	2543.353292	5.862733	-0.025798	2.788672
130.085525	2551.427252	5.867738	-0.025845	2.792774
130.479972	2559.421272	5.872742	-0.025924	2.796840
131.043748	2567.461399	5.877747	-0.026034	2.800934
131.167985	2575.478223	5.882752	-0.026062	2.804984
131.335174	2583.543333	5.887757	-0.026099	2.809054
131.645594	2591.611223	5.892762	-0.026162	2.813129
131.820054	2599.657445	5.897766	-0.026199	2.817179
132.180520	2607.697143	5.902771	-0.026272	2.821230
132.452943	2615.707508	5.907776	-0.026328	2.825256
132.661062	2623.770551	5.912781	-0.026372	2.829299
132.885389	2631.865933	5.917786	-0.026419	2.833353
133.185879	2639.874116	5.922790	-0.026480	2.837362
133.793698	2647.864515	5.927795	-0.026598	2.841373
133.626114	2655.929393	5.932800	-0.026572	2.845373
133.811488	2663.963663	5.937805	-0.026612	2.849371
134.185210	2672.022067	5.942810	-0.026687	2.853386
134.201887	2680.073006	5.947814	-0.026695	2.857372
134.485133	2688.108958	5.952819	-0.026753	2.861360
134.791402	2696.120145	5.957824	-0.026816	2.865331
135.113089	2704.157369	5.962829	-0.026881	2.869310
135.402140	2712.248947	5.967834	-0.026940	2.873309
135.513627	2720.266957	5.972838	-0.026966	2.877256
135.964994	2728.282263	5.977843	-0.027055	2.881215
135.918070	2736.345931	5.982848	-0.027052	2.885165
136.383113	2744.353426	5.987853	-0.027144	2.889110
136.377514	2752.448075	5.992858	-0.027148	2.893067
136.471137	2760.494803	5.997862	-0.027170	2.897000
137.077779	2768.503404	6.002867	-0.027289	2.900936
137.222964	2776.530592	6.007872	-0.027321	2.904852
137.387378	2784.591637	6.012877	-0.027357	2.908780
137.606404	2792.708494	6.017882	-0.027403	2.912732
137.865335	2800.726440	6.022886	-0.027456	2.916634
138.070841	2808.746292	6.027891	-0.027500	2.920528
138.166443	2816.744427	6.032896	-0.027523	2.924400
138.431531	2824.788381	6.037901	-0.027578	2.928299
138.697787	2832.828177	6.042906	-0.027632	2.932190
138.834075	2840.874805	6.047910	-0.027663	2.936072
139.399280	2848.862120	6.052915	-0.027773	2.939944
139.542448	2856.893094	6.057920	-0.027805	2.943809
139.839938	2864.945982	6.062925	-0.027866	2.947687
140.199618	2872.993132	6.067930	-0.027938	2.951561
140.491250	2881.024448	6.072934	-0.027998	2.955419
140.814157	2889.053894	6.077939	-0.028063	2.959272
140.840667	2897.102313	6.082944	-0.028073	2.963114
141.164110	2905.120780	6.087949	-0.028139	2.966952
141.782003	2913.163526	6.092954	-0.028259	2.970811
142.121871	2921.204760	6.097958	-0.028328	2.974650
142.280735	2929.249584	6.102963	-0.028362	2.978477
142.434900	2937.304688	6.107968	-0.028396	2.982304
142.654379	2945.336882	6.112973	-0.028443	2.986118
142.922859	2953.384833	6.117978	-0.028498	2.989937
143.161521	2961.460276	6.122982	-0.028548	2.993763
143.310611	2969.479495	6.127987	-0.028581	2.997553
143.582752	2977.495946	6.132992	-0.028636	3.001343
143.730310	2985.488673	6.137997	-0.028669	3.005110
144.129197	2993.542844	6.143002	-0.028749	3.008914
144.403003	3001.569975	6.148006	-0.028805	3.012695
144.535102	3009.660861	6.153011	-0.028835	3.016493
144.805817	3017.665423	6.158016	-0.028890	3.020253
145.049502	3025.671572	6.163021	-0.028941	3.024008
145.210672	3033.735217	6.168026	-0.028976	3.027781
145.377062	3041.774304	6.173030	-0.029013	3.031538
145.581879	3049.830196	6.178035	-0.029056	3.035300
145.602584	3057.849478	6.183040	-0.029065	3.039032
145.810781	3065.863932	6.188045	-0.029109	3.042765
146.536656	3073.871209	6.193050	-0.029249	3.046516
146.424670	3081.923243	6.198054	-0.029234	3.050242
146.694911	3089.995669	6.203059	-0.029289	3.053992
147.149310	3098.001808	6.208064	-0.029379	3.057715
147.303180	3106.051470	6.213069	-0.029413	3.061439
147.774431	3114.052120	6.218074	-0.029506	3.065151
148.081082	3122.084957	6.223078	-0.029569	3.068866
148.381848	3130.197553	6.228083	-0.029630	3.072612
148.614346	3138.271412	6.233088	-0.029678	3.076333
148.775094	3146.231091	6.238093	-0.029714	3.079993
148.970782	3154.267660	6.243098	-0.029755	3.083686
148.854687	3162.299801	6.248102	-0.029739	3.087358
149.183560	3170.342287	6.253107	-0.029805	3.091051
149.523901	3178.375629	6.258112	-0.029874	3.094736
149.554061	3186.403366	6.263117	-0.029885	3.098400
149.875607	3194.428510	6.268122	-0.029950	3.102071
150.170292	3202.437197	6.273126	-0.030010	3.105730
150.466701	3210.484861	6.278131	-0.030070	3.109402
150.607837	3218.538429	6.283136	-0.030102	3.113065
150.712511	3226.575574	6.288141	-0.030127	3.116714
151.192224	3234.572500	6.293146	-0.030221	3.120358
151.408986	3242.576117	6.298150	-0.030267	3.123989
151.494455	3250.651243	6.303155	-0.030288	3.127642
151.878845	3258.666868	6.308160	-0.030365	3.131278
151.976116	3266.715481	6.313165	-0.030388	3.134911
152.190526	3274.781379	6.318170	-0.030433	3.138552
152.466352	3282.770166	6.323174	-0.030490	3.142158
153.034212	3290.792480	6.328179	-0.030601	3.145787
152.981958	3298.837008	6.333184	-0.030597	3.149395
153.319361	3306.893800	6.338189	-0.030665	3.153021
153.827514	3314.931541	6.343194	-0.030765	3.156642
153.946167	3322.926555	6.348198	-0.030792	3.160223
154.082803	3330.956230	6.353203	-0.030823	3.163816
154.351121	3338.979548	6.358208	-0.030878	3.167407
154.589684	3347.015692	6.363213	-0.030927	3.170999
154.828041	3355.099688	6.368218	-0.030977	3.174608
155.206048	3363.067865	6.373222	-0.031053	3.178167
155.583757	3371.113416	6.378227	-0.031128	3.181757
155.666268	3379.169103	6.383232	-0.031149	3.185335
155.904026	3387.207051	6.388237	-0.031198	3.188907
156.265583	3395.249370	6.393242	-0.031271	3.192482
156.423638	3403.308280	6.398246	-0.031306	3.196052
156.652033	3411.281894	6.403251	-0.031353	3.199583
156.966302	3419.286730	6.408256	-0.031417	3.203128
157.386572	3427.316780	6.413261	-0.031501	3.206684
157.609481	3435.383136	6.418266	-0.031547	3.210245
157.829943	3443.419010	6.423270	-0.031594	3.213787
157.856819	3451.497741	6.428275	-0.031604	3.217336
158.141425	3459.485725	6.433280	-0.031662	3.220853
158.237524	3467.483868	6.438285	-0.031685	3.224362
158.550558	3475.549683	6.443290	-0.031749	3.227906
158.806244	3483.589162	6.448294	-0.031802	3.231432
159.114621	3491.664110	6.453299	-0.031864	3.234971
159.337399	3499.640760	6.458304	-0.031911	3.238461
159.433071	3507.667306	6.463309	-0.031934	3.241963
159.665272	3515.672725	6.468314	-0.031983	3.245458
159.625882	3523.717017	6.473318	-0.031981	3.248955
159.983388	3531.756375	6.478323	-0.032052	3.252462
160.271375	3539.788675	6.483328	-0.032111	3.255959
160.342199	3547.777641	6.488333	-0.032130	3.259425
160.408694	3555.865716	6.493338	-0.032147	3.262930
160.694798	3563.855796	6.498342	-0.032206	3.266398
160.772772	3571.924102	6.503347	-0.032226	3.269887
161.128000	3579.955569	6.508352	-0.032297	3.273368
161.302506	3587.973787	6.513357	-0.032335	3.276832
161.519261	3596.013432	6.518362	-0.032380	3.280304
161.383699	3604.019524	6.523366	-0.032360	3.283743
161.845779	3612.024339	6.528371	-0.032452	3.287202
161.902750	3620.090307	6.533376	-0.032468	3.290667
162.021417	3628.126496	6.538381	-0.032495	3.294118
162.369065	3636.149185	6.543386	-0.032565	3.297569
162.609377	3644.146268	6.548390	-0.032615	3.301001
162.477739	3652.195235	6.553395	-0.032596	3.304438
162.796222	3660.212422	6.558400	-0.032660	3.307874
162.990372	3668.246963	6.563405	-0.032702	3.311309
163.238312	3676.340143	6.568410	-0.032753	3.314768
163.231728	3684.315503	6.573414	-0.032757	3.318164
163.579577	3692.333095	6.578419	-0.032827	3.321587
163.664327	3700.347764	6.583424	-0.032848	3.324996
163.800272	3708.372827	6.588429	-0.032879	3.328407
164.011682	3716.442301	6.593434	-0.032923	3.331837
164.236655	3724.439369	6.598438	-0.032970	3.335232
164.517314	3732.461984	6.603443	-0.033028	3.338638
164.364924	3740.526975	6.608448	-0.033005	3.342041
164.740309	3748.506890	6.613453	-0.033080	3.345425
164.988037	3756.566862	6.618458	-0.033131	3.348834
165.123436	3764.616731	6.623462	-0.033162	3.352231
165.214875	3772.681602	6.628467	-0.033184	3.355630
165.420569	3780.651275	6.633472	-0.033227	3.358989
165.596593	3788.681391	6.638477	-0.033265	3.362369
165.676520	3796.718993	6.643482	-0.033286	3.365746
165.910575	3804.737365	6.648486	-0.033334	3.369116
166.083923	3812.790694	6.653491	-0.033372	3.372496
166.192262	3820.847279	6.658496	-0.033397	3.375871
166.261265	3828.839862	6.663501	-0.033415	3.379215
166.593096	3836.875702	6.668506	-0.033483	3.382583
166.625675	3844.889633	6.673510	-0.033494	3.385927
166.715918	3852.910390	6.678515	-0.033516	3.389273
167.007233	3860.991203	6.683520	-0.033575	3.392648
167.210507	3869.072588	6.688525	-0.033619	3.396017
167.300405	3877.038560	6.693530	-0.033640	3.399330
167.658622	3885.020758	6.698534	-0.033712	3.402656
167.902267	3893.034813	6.703539	-0.033763	3.405988
167.988759	3901.038258	6.708544	-0.033784	3.409307
168.093443	3909.087279	6.713549	-0.033809	3.412643
168.488676	3917.129974	6.718554	-0.033888	3.415982
168.474750	3925.114751	6.723558	-0.033891	3.419280
168.648539	3933.154573	6.728563	-0.033928	3.422604
169.222949	3941.150397	6.733568	-0.034040	3.425920
169.246848	3949.200192	6.738573	-0.034050	3.429237
169.633128	3957.252414	6.743578	-0.034127	3.432563
169.833988	3965.274596	6.748582	-0.034170	3.435868
169.930703	3973.317654	6.753587	-0.034193	3.439174
170.121225	3981.341085	6.758592	-0.034234	3.442473
170.271370	3989.332147	6.763597	-0.034267	3.445753
170.451984	3997.390218	6.768602	-0.034306	3.449059
170.511689	4005.412429	6.773606	-0.034322	3.452343
170.693765	4013.468377	6.778611	-0.034361	3.455642
170.962396	4021.476970	6.783616	-0.034417	3.458921
171.215482	4029.480759	6.788621	-0.034469	3.462195
171.393113	4037.504411	6.793626	-0.034507	3.465470
171.465669	4045.541056	6.798630	-0.034526	3.468745
171.589554	4053.605823	6.803635	-0.034554	3.472030
171.607827	4061.668996	6.808640	-0.034563	3.475307
171.812090	4069.643528	6.813645	-0.034606	3.478552
172.154176	4077.664773	6.818650	-0.034675	3.481816
172.060783	4085.677919	6.823654	-0.034663	3.485061
172.389167	4093.669209	6.828659	-0.034730	3.488307
172.568022	4101.713798	6.833664	-0.034768	3.491566
172.611151	4109.759604	6.838669	-0.034781	3.494819
172.853208	4117.785812	6.843674	-0.034832	3.498067
173.057702	4125.799291	6.848678	-0.034875	3.501306
173.333233	4133.789976	6.853683	-0.034932	3.504535
173.593394	4141.823489	6.858688	-0.034985	3.507777
173.584672	4149.874453	6.863693	-0.034989	3.511015
173.836436	4157.900354	6.868698	-0.035041	3.514249
173.894853	4165.919840	6.873702	-0.035057	3.517470
174.307086	4173.944514	6.878707	-0.035139	3.520702
174.482927	4181.951961	6.883712	-0.035177	3.523916
174.789010	4189.941275	6.888717	-0.035239	3.527124
174.820098	4198.051841	6.893722	-0.035250	3.530370
175.091799	4206.066452	6.898726	-0.035306	3.533581
175.203228	4214.108434	6.903731	-0.035332	3.536795
175.308462	4222.131638	6.908736	-0.035357	3.539999
175.559011	4230.137904	6.913741	-0.035409	3.543198
175.778307	4238.196230	6.918746	-0.035455	3.546413
175.827549	4246.213472	6.923750	-0.035469	3.549604
176.004412	4254.303079	6.928755	-0.035508	3.552825
176.224272	4262.338708	6.933760	-0.035554	3.556022
176.666182	4270.275435	6.938765	-0.035641	3.559184
176.727088	4278.305968	6.943770	-0.035658	3.562369
176.845462	4286.287424	6.948774	-0.035685	3.565534
177.260572	4294.302309	6.953779	-0.035768	3.568717
177.436921	4302.366593	6.958784	-0.035806	3.571910
177.395461	4310.403541	6.963789	-0.035803	3.575084
177.591226	4318.433435	6.968794	-0.035845	3.578258
177.842059	4326.422177	6.973798	-0.035897	3.581415
178.050429	4334.417213	6.978803	-0.035941	3.584570
178.318587	4342.478546	6.983808	-0.035996	3.587751
178.521075	4350.470098	6.988813	-0.036039	3.590899
178.924850	4358.527380	6.993818	-0.036120	3.594076
178.898715	4366.545732	6.998822	-0.036120	3.597223
179.022573	4374.543612	7.003827	-0.036148	3.600363
179.158382	4382.570001	7.008832	-0.036179	3.603512
179.214481	4390.611561	7.013837	-0.036194	3.606661
179.728666	4398.606016	7.018842	-0.036295	3.609803
180.139375	4406.662175	7.023846	-0.036377	3.612963
180.313476	4414.679934	7.028851	-0.036415	3.616098
180.752106	4422.666849	7.033856	-0.036502	3.619226
180.917831	4430.693712	7.038861	-0.036538	3.622359
181.256151	4438.739551	7.043866	-0.036606	3.625502
181.234076	4446.765585	7.048870	-0.036607	3.628624
181.477396	4454.831419	7.053875	-0.036658	3.631766
181.681785	4462.893396	7.058880	-0.036701	3.634903
182.023312	4470.861168	7.063885	-0.036770	3.638005
182.481507	4478.879374	7.068890	-0.036860	3.641126
182.570455	4486.851157	7.073894	-0.036882	3.644217
182.414270	4494.922476	7.078899	-0.036858	3.647337
182.753044	4502.950515	7.083904	-0.036927	3.650451
183.033593	4510.982280	7.088909	-0.036984	3.653562
183.281563	4519.055606	7.093914	-0.037036	3.656686
183.415232	4527.015806	7.098918	-0.037066	3.659760
183.637964	4535.024531	7.103923	-0.037112	3.662853
183.926229	4543.074627	7.108928	-0.037171	3.665960
184.044140	4551.109904	7.113933	-0.037199	3.669055
184.353043	4559.169234	7.118938	-0.037261	3.672161
184.497504	4567.167694	7.123942	-0.037294	3.675237
184.812085	4575.184334	7.128947	-0.037357	3.678322
184.839638	4583.222921	7.133952	-0.037368	3.681406
184.865612	4591.159141	7.138957	-0.037378	3.684447
185.325319	4599.235528	7.143962	-0.037469	3.687551
185.283637	4607.283492	7.148966	-0.037466	3.690628
185.455446	4615.275055	7.153971	-0.037503	3.693687
185.854426	4623.314012	7.158976	-0.037583	3.696767
185.804563	4631.311504	7.163981	-0.037579	3.699817
185.882115	4639.358050	7.168986	-0.037598	3.702886
186.049054	4647.375155	7.173990	-0.037635	3.705944
186.312688	4655.370525	7.178995	-0.037689	3.708994
186.531500	4663.451062	7.184000	-0.037735	3.712072
186.551344	4671.514265	7.189005	-0.037744	3.715136
186.857494	4679.503193	7.194010	-0.037806	3.718177
187.100619	4687.501199	7.199014	-0.037857	3.721217
187.270663	4695.488285	7.204019	-0.037894	3.724248
187.664770	4703.519628	7.209024	-0.037972	3.727299
187.589771	4711.528132	7.214029	-0.037964	3.730328
187.948583	4719.553618	7.219034	-0.038036	3.733371
188.008982	4727.605502	7.224038	-0.038052	3.736414
188.248102	4735.579914	7.229043	-0.038102	3.739430
188.526132	4743.635443	7.234048	-0.038159	3.742475
188.849404	4751.620242	7.239053	-0.038224	3.745492
189.053180	4759.715301	7.244058	-0.038268	3.748545
189.092440	4767.740129	7.249062	-0.038280	3.751565
189.248019	4775.746788	7.254067	-0.038314	3.754579
189.466546	4783.815097	7.259072	-0.038360	3.757615
189.438745	4791.782061	7.264077	-0.038360	3.760604
189.710671	4799.773587	7.269082	-0.038416	3.763608
189.826509	4807.854527	7.274086	-0.038443	3.766638
189.994755	4815.831231	7.279091	-0.038480	3.769629
190.353037	4823.899623	7.284096	-0.038552	3.772656
190.410765	4831.917697	7.289101	-0.038568	3.775655
190.716062	4839.937242	7.294106	-0.038630	3.778657
190.700700	4847.987654	7.299110	-0.038632	3.781661
190.954057	4855.947926	7.304115	-0.038684	3.784636
191.477370	4864.014076	7.309120	-0.038787	3.787653
191.549847	4872.002241	7.314125	-0.038806	3.790629
191.939214	4880.059299	7.319130	-0.038884	3.793635
192.129511	4888.094403	7.324134	-0.038924	3.796626
192.736886	4896.017111	7.329139	-0.039043	3.799582
192.902492	4904.081677	7.334144	-0.039079	3.802579
192.934221	4912.076328	7.339149	-0.039090	3.805545
193.182301	4920.129473	7.344154	-0.039141	3.808535
193.454811	4928.122689	7.349158	-0.039197	3.811500
193.494270	4936.154372	7.354163	-0.039210	3.814473
193.834034	4944.202827	7.359168	-0.039278	3.817455
193.884342	4952.207651	7.364173	-0.039293	3.820413
194.072507	4960.219237	7.369178	-0.039333	3.823375
194.118186	4968.266464	7.374182	-0.039347	3.826344
194.359000	4976.243562	7.379187	-0.039397	3.829289
194.572063	4984.357405	7.384192	-0.039442	3.832281
194.553866	4992.323609	7.389197	-0.039444	3.835212
194.909761	5000.347795	7.394202	-0.039515	3.838170
195.088040	5008.358591	7.399206	-0.039554	3.841117
194.898065	5016.338462	7.404211	-0.039524	3.844042
195.215364	5024.387035	7.409216	-0.039588	3.847001
195.417205	5032.364890	7.414221	-0.039631	3.849930
195.814424	5040.465105	7.419226	-0.039710	3.852905
195.816591	5048.485269	7.424230	-0.039716	3.855840
196.014375	5056.484526	7.429235	-0.039758	3.858769
196.245781	5064.571008	7.434240	-0.039806	3.861729
196.378883	5072.532337	7.439245	-0.039836	3.864639
196.945696	5080.591598	7.444250	-0.039947	3.867591
197.120953	5088.574924	7.449254	-0.039985	3.870505
197.171983	5096.829992	7.454259	-0.040000	3.873513
197.326646	5104.866268	7.459264	-0.040034	3.876442
197.489236	5112.707352	7.464269	-0.040069	3.879297
197.665645	5120.732271	7.469274	-0.040107	3.882217
197.953757	5128.687693	7.474278	-0.040166	3.885112
198.158206	5136.702686	7.479283	-0.040209	3.888025
198.374144	5144.747288	7.484288	-0.040255	3.890947
198.491435	5152.738613	7.489293	-0.040282	3.893845
198.640259	5160.815362	7.494298	-0.040315	3.896772
198.794534	5168.775404	7.499302	-0.040349	3.899655
198.758842	5176.810943	7.504307	-0.040347	3.902560
198.926319	5184.876455	7.509312	-0.040384	3.905477
199.149475	5192.853489	7.514317	-0.040431	3.908362
199.263433	5200.891510	7.519322	-0.040457	3.911263
199.417954	5208.916139	7.524326	-0.040491	3.914159
199.678138	5216.935293	7.529331	-0.040545	3.917053
199.857036	5224.903914	7.534336	-0.040583	3.919924
200.077904	5232.928421	7.539341	-0.040630	3.922815
200.524126	5240.935353	7.544346	-0.040718	3.925700
200.594077	5248.983040	7.549350	-0.040736	3.928592
200.702210	5256.997351	7.554355	-0.040762	3.931470
200.956926	5265.055525	7.559360	-0.040814	3.934365
201.135318	5273.018978	7.564365	-0.040853	3.937222
201.435283	5281.057255	7.569370	-0.040914	3.940105
201.396688	5289.087786	7.574374	-0.040912	3.942978
201.532321	5297.097222	7.579379	-0.040942	3.945845
201.617868	5305.112388	7.584384	-0.040964	3.948710
201.609100	5313.150283	7.589389	-0.040967	3.951580
202.004468	5321.218080	7.594394	-0.041046	3.954465
202.254898	5329.221023	7.599398	-0.041098	3.957323
202.199145	5337.164906	7.604403	-0.041093	3.960152
202.828910	5345.187563	7.609408	-0.041215	3.963019
203.022791	5353.209134	7.614413	-0.041257	3.965876
203.103044	5361.243767	7.619418	-0.041277	3.968733
203.251002	5369.287164	7.624422	-0.041310	3.971593
203.780350	5377.294590	7.629427	-0.041413	3.974444
204.006582	5385.343441	7.634432	-0.041461	3.977303
204.045108	5393.304806	7.639437	-0.041473	3.980126
204.205787	5401.385159	7.644442	-0.041508	3.982990
204.346497	5409.373510	7.649446	-0.041540	3.985820
204.359384	5417.407096	7.654451	-0.041547	3.988662
204.566500	5425.449811	7.659456	-0.041591	3.991508
204.771340	5433.457790	7.664461	-0.041635	3.994340
205.036954	5441.505040	7.669466	-0.041689	3.997184
205.244938	5449.494358	7.674470	-0.041733	4.000005
205.413825	5457.512456	7.679475	-0.041770	4.002834
205.599805	5465.549718	7.684480	-0.041810	4.005667
205.746786	5473.531509	7.689485	-0.041842	4.008479
206.108523	5481.585705	7.694490	-0.041915	4.011317
206.299687	5489.646280	7.699494	-0.041956	4.014152
206.411075	5497.666389	7.704499	-0.041982	4.016971
206.575201	5505.667600	7.709504	-0.042018	4.019781
206.606613	5513.674105	7.714509	-0.042029	4.022589
206.859621	5521.685408	7.719514	-0.042081	4.025401
207.111460	5529.708719	7.724518	-0.042133	4.028214
207.419681	5537.730837	7.729523	-0.042196	4.031026
207.748880	5545.867635	7.734528	-0.042262	4.033877
207.569437	5553.843695	7.739533	-0.042234	4.036661
207.899097	5561.777401	7.744538	-0.042301	4.039437
208.271477	5569.822278	7.749542	-0.042375	4.042250
208.162471	5577.775184	7.754547	-0.042360	4.045021
208.200258	5585.839316	7.759552	-0.042373	4.047832
208.453203	5593.834537	7.764557	-0.042425	4.050620
208.638664	5601.870519	7.769562	-0.042465	4.053419
208.793987	5609.927770	7.774566	-0.042499	4.056223
208.923896	5617.865907	7.779571	-0.042528	4.058984
209.097105	5625.955205	7.784576	-0.042566	4.061795
209.362413	5633.891606	7.789581	-0.042620	4.064553
209.480096	5641.969245	7.794586	-0.042648	4.067356
209.841421	5649.954259	7.799590	-0.042720	4.070129
210.042170	5658.004600	7.804595	-0.042763	4.072919
210.200202	5666.047841	7.809600	-0.042797	4.075705
210.267161	5674.014531	7.814605	-0.042815	4.078461
210.487699	5682.028393	7.819610	-0.042861	4.081234
210.826532	5690.032242	7.824614	-0.042930	4.084003
211.005958	5698.096853	7.829619	-0.042968	4.086789
211.452155	5706.058733	7.834624	-0.043057	4.089541
211.221369	5714.137907	7.839629	-0.043019	4.092322
211.327332	5722.188488	7.844634	-0.043044	4.095096
211.450678	5730.197627	7.849638	-0.043072	4.097855
211.759182	5738.187813	7.854643	-0.043135	4.100607
211.932145	5746.197802	7.859648	-0.043172	4.103362
212.000540	5754.180885	7.864653	-0.043190	4.106105
212.253763	5762.254199	7.869658	-0.043243	4.108880
212.421277	5770.309016	7.874662	-0.043279	4.111645
212.454679	5778.327009	7.879667	-0.043291	4.114394
212.901809	5786.404168	7.884672	-0.043379	4.117167
213.050691	5794.295553	7.889677	-0.043412	4.119870
213.155390	5802.355413	7.894682	-0.043437	4.122629
213.294196	5810.356430	7.899686	-0.043468	4.125366
213.341086	5818.353402	7.904691	-0.043482	4.128098
213.596277	5826.433165	7.909696	-0.043535	4.130860
213.865679	5834.472165	7.914701	-0.043590	4.133606
213.994143	5842.516225	7.919706	-0.043619	4.136350
214.135505	5850.475399	7.924710	-0.043651	4.139064
214.265732	5858.517303	7.929715	-0.043680	4.141804
214.728099	5866.492216	7.934720	-0.043771	4.144523
214.899707	5874.545292	7.939725	-0.043809	4.147264
214.915192	5882.555038	7.944730	-0.043817	4.149986
215.000508	5890.591526	7.949734	-0.043838	4.152716
215.407245	5898.622174	7.954739	-0.043919	4.155446
215.536302	5906.676164	7.959744	-0.043948	4.158179
215.473962	5914.615851	7.964749	-0.043942	4.160869
215.685841	5922.600156	7.969754	-0.043986	4.163576
215.755598	5930.658244	7.974758	-0.044005	4.166305
216.027131	5938.619737	7.979763	-0.044060	4.169001
216.258767	5946.715336	7.984768	-0.044109	4.171740
216.429206	5954.727805	7.989773	-0.044146	4.174449
216.426857	5962.720763	7.994778	-0.044151	4.177147
216.834498	5970.777569	7.999782	-0.044232	4.179870
217.109656	5978.744109	8.004787	-0.044288	4.182559
217.045060	5986.766833	8.009792	-0.044281	4.185261
217.209295	5994.785450	8.014797	-0.044317	4.187963
217.417674	6002.819035	8.019802	-0.044361	4.190668
217.480279	6010.929441	8.024806	-0.044378	4.193396
217.680547	6018.922756	8.029811	-0.044421	4.196085
217.766034	6026.910040	8.034816	-0.044442	4.198768
218.030507	6034.875445	8.039821	-0.044496	4.201444
217.979270	6042.868946	8.044826	-0.044492	4.204125
218.294370	6050.890631	8.049830	-0.044556	4.206817
218.328504	6058.902022	8.054835	-0.044568	4.209501
218.434165	6066.978859	8.059840	-0.044593	4.212206
218.459661	6074.980299	8.064845	-0.044602	4.214883
218.817190	6082.983329	8.069850	-0.044674	4.217562
219.012269	6090.961905	8.074854	-0.044716	4.220230
218.947567	6098.992663	8.079859	-0.044709	4.222911
219.143619	6107.022634	8.084864	-0.044751	4.225592
219.361770	6115.041222	8.089869	-0.044797	4.228268
219.316167	6123.049288	8.094874	-0.044793	4.230937
219.448975	6131.124718	8.099878	-0.044823	4.233628
219.487812	6139.124558	8.104883	-0.044836	4.236291
219.975611	6147.101537	8.109888	-0.044932	4.238949
220.071481	6155.124034	8.114893	-0.044955	4.241617
220.391591	6163.091691	8.119898	-0.045020	4.244267
220.420422	6171.180837	8.124902	-0.045030	4.246952
220.586438	6179.169634	8.129907	-0.045067	4.249605
220.845591	6187.270167	8.134912	-0.045120	4.252293
220.911586	6195.250260	8.139917	-0.045138	4.254938
221.134099	6203.287654	8.144922	-0.045184	4.257602
221.026301	6211.280647	8.149926	-0.045169	4.260246
221.098276	6219.296382	8.154931	-0.045188	4.262898
221.334048	6227.280635	8.159936	-0.045237	4.265539
221.336380	6235.358396	8.164941	-0.045243	4.268207
221.535018	6243.375496	8.169946	-0.045285	4.270856
221.935346	6251.455800	8.174950	-0.045365	4.273525
221.983163	6259.427357	8.179955	-0.045379	4.276154
222.172874	6267.450416	8.184960	-0.045420	4.278799
222.450740	6275.444023	8.189965	-0.045477	4.281434
222.426962	6283.399095	8.194970	-0.045477	4.284051
222.544671	6291.477003	8.199974	-0.045505	4.286709
222.689680	6299.434831	8.204979	-0.045537	4.289326
222.901163	6307.554702	8.209984	-0.045581	4.291995
223.066019	6315.530563	8.214989	-0.045617	4.294615
223.134257	6323.558468	8.219994	-0.045635	4.297249
223.449330	6331.572968	8.224998	-0.045699	4.299879
223.385211	6339.556836	8.230003	-0.045693	4.302495
223.564911	6347.573104	8.235008	-0.045731	4.305122
223.807924	6355.584262	8.240013	-0.045782	4.307745
223.909076	6363.617106	8.245018	-0.045806	4.310373
224.069678	6371.670715	8.250022	-0.045841	4.313007
224.033351	6379.670769	8.255027	-0.045839	4.315620
224.371766	6387.700569	8.260032	-0.045908	4.318244
224.455817	6395.686610	8.265037	-0.045929	4.320851
224.716182	6403.680252	8.270042	-0.045982	4.323459
224.974423	6411.734464	8.275046	-0.046036	4.326085
224.984444	6419.688895	8.280051	-0.046043	4.328676
225.133561	6427.797613	8.285056	-0.046076	4.331316
225.382254	6435.817978	8.290061	-0.046127	4.333927
225.485212	6443.813760	8.295066	-0.046152	4.336527
225.553480	6451.825702	8.300070	-0.046170	4.339130
225.664351	6459.813699	8.305075	-0.046195	4.341725
226.077340	6467.802124	8.310080	-0.046278	4.344320
226.124347	6475.870500	8.315085	-0.046292	4.346937
226.155135	6483.871829	8.320090	-0.046303	4.349530
226.445170	6491.914136	8.325094	-0.046362	4.352137
226.629400	6500.005971	8.330099	-0.046401	4.354758
226.740070	6508.036658	8.335104	-0.046427	4.357356
226.780340	6515.948982	8.340109	-0.046440	4.359915
226.904552	6523.882697	8.345114	-0.046468	4.362479
227.100855	6531.930949	8.350118	-0.046510	4.365080
227.456093	6539.959750	8.355123	-0.046581	4.367673
227.862732	6547.980878	8.360128	-0.046662	4.370263
227.682235	6556.011189	8.365133	-0.046634	4.372850
228.003348	6564.051401	8.370138	-0.046699	4.375442
228.260919	6572.020093	8.375142	-0.046752	4.378010
228.436133	6580.053303	8.380147	-0.046790	4.380596
228.530239	6588.078231	8.385152	-0.046813	4.383177
228.609472	6596.063504	8.390157	-0.046833	4.385744
228.938832	6604.127838	8.395162	-0.046899	4.388336
229.180576	6612.149966	8.400166	-0.046950	4.390913
229.380172	6620.163035	8.405171	-0.046992	4.393485
229.447865	6628.249365	8.410176	-0.047010	4.396078
229.518242	6636.182581	8.415181	-0.047028	4.398620
229.541435	6644.198243	8.420186	-0.047038	4.401187
229.832861	6652.224921	8.425190	-0.047097	4.403758
229.951349	6660.207482	8.430195	-0.047125	4.406312
230.031215	6668.258845	8.435200	-0.047145	4.408887
230.276696	6676.253680	8.440205	-0.047196	4.411442
230.558021	6684.314308	8.445210	-0.047253	4.414018
230.653650	6692.375788	8.450214	-0.047276	4.416591
230.654802	6700.319110	8.455219	-0.047282	4.419124
230.905369	6708.410188	8.460224	-0.047334	4.421705
230.981928	6716.336165	8.465229	-0.047353	4.424230
231.072758	6724.398911	8.470234	-0.047375	4.426798
231.499638	6732.437952	8.475238	-0.047460	4.429358
231.381716	6740.449359	8.480243	-0.047443	4.431905
231.411842	6748.520233	8.485248	-0.047454	4.434470
231.517727	6756.540674	8.490253	-0.047479	4.437018
231.729696	6764.476771	8.495258	-0.047524	4.439539
231.962130	6772.531365	8.500262	-0.047572	4.442095
231.851555	6780.434749	8.505267	-0.047557	4.444601
232.160025	6788.509489	8.510272	-0.047620	4.447161
232.403131	6796.546478	8.515277	-0.047670	4.449708
232.527061	6804.561086	8.520282	-0.047699	4.452246
232.550772	6812.630937	8.525286	-0.047708	4.454799
232.867709	6820.606992	8.530291	-0.047772	4.457322
233.036459	6828.623104	8.535296	-0.047809	4.459856
233.124983	6836.626023	8.540301	-0.047831	4.462384
233.354124	6844.625929	8.545306	-0.047879	4.464910
233.534158	6852.666671	8.550310	-0.047918	4.467447
233.634002	6860.661470	8.555315	-0.047941	4.469968
233.896200	6868.715502	8.560320	-0.047995	4.472507
234.158937	6876.727610	8.565325	-0.048050	4.475031
234.186175	6884.733008	8.570330	-0.048060	4.477551
234.214742	6892.762775	8.575335	-0.048070	4.480077
234.354477	6900.730376	8.580339	-0.048102	4.482582
234.497171	6908.743215	8.585344	-0.048133	4.485100
234.564711	6916.798170	8.590349	-0.048151	4.487630
234.763766	6924.793725	8.595354	-0.048194	4.490140
234.930250	6932.850902	8.600359	-0.048230	4.492668
234.997829	6940.805048	8.605363	-0.048248	4.495162
235.267997	6948.857451	8.610368	-0.048303	4.497686
235.522331	6956.822888	8.615373	-0.048356	4.500181
235.754130	6964.886848	8.620378	-0.048404	4.502705
236.087647	6972.908625	8.625383	-0.048472	4.505215
236.063159	6980.902088	8.630387	-0.048472	4.507714
236.200724	6988.950615	8.635392	-0.048503	4.510229
236.197895	6996.990832	8.640397	-0.048508	4.512740
236.676676	7005.066756	8.645402	-0.048602	4.515262
236.690853	7013.008797	8.650407	-0.048610	4.517739
236.799633	7020.980546	8.655411	-0.048636	4.520224
236.947283	7029.014582	8.660416	-0.048668	4.522728
237.033352	7037.000422	8.665421	-0.048690	4.525215
237.114873	7045.005779	8.670426	-0.048710	4.527707
237.335931	7053.009628	8.675431	-0.048756	4.530197
237.531308	7061.075400	8.680435	-0.048798	4.532705
237.686958	7069.106778	8.685440	-0.048832	4.535200
237.889653	7077.095095	8.690445	-0.048875	4.537681
237.989772	7085.071375	8.695450	-0.048899	4.540157
238.089109	7093.143674	8.700455	-0.048923	4.542661
238.132072	7101.094875	8.705459	-0.048936	4.545126
238.432150	7109.171997	8.710464	-0.048997	4.547630
238.735603	7117.145777	8.715469	-0.049059	4.550099
238.825944	7125.220927	8.720474	-0.049081	4.552599
238.950987	7133.246888	8.725479	-0.049109	4.555082
239.130620	7141.222491	8.730483	-0.049148	4.557548
239.251456	7149.192642	8.735488	-0.049176	4.560011
239.370108	7157.263229	8.740493	-0.049203	4.562504
239.546502	7165.235867	8.745498	-0.049241	4.564965
239.747475	7173.327180	8.750503	-0.049284	4.567461
239.635724	7181.289426	8.755507	-0.049268	4.569916
240.067693	7189.349320	8.760512	-0.049354	4.572400
240.291886	7197.355634	8.765517	-0.049401	4.574866
240.351533	7205.383093	8.770522	-0.049417	4.577337
240.530888	7213.393265	8.775527	-0.049456	4.579802
240.795409	7221.404560	8.780531	-0.049511	4.582265
240.889402	7229.409515	8.785536	-0.049533	4.584725
240.940368	7237.454495	8.790541	-0.049548	4.587196
240.981238	7245.494706	8.795546	-0.049561	4.589665
241.228749	7253.530744	8.800551	-0.049612	4.592130
241.387687	7261.513305	8.805555	-0.049647	4.594578
241.595149	7269.569409	8.810560	-0.049691	4.597048
241.642044	7277.497606	8.815565	-0.049705	4.599476
241.837688	7285.531860	8.820570	-0.049746	4.601936
241.992208	7293.526649	8.825575	-0.049780	4.604382
242.167621	7301.577819	8.830579	-0.049818	4.606845
242.361274	7309.559806	8.835584	-0.049860	4.609285
242.473713	7317.601327	8.840589	-0.049886	4.611741
242.618024	7325.601161	8.845594	-0.049918	4.614184
242.725427	7333.659530	8.850599	-0.049943	4.616643
242.709450	7341.623920	8.855603	-0.049945	4.619072
242.865040	7349.679660	8.860608	-0.049980	4.621528
242.961866	7357.653619	8.865613	-0.050003	4.623958
243.203423	7365.661682	8.870618	-0.050053	4.626396
243.614848	7373.692722	8.875623	-0.050135	4.628840
243.737202	7381.730889	8.880627	-0.050163	4.631286
243.955953	7389.787880	8.885632	-0.050209	4.633735
244.017490	7397.814027	8.890637	-0.050226	4.636174
243.994895	7405.745568	8.895642	-0.050227	4.638583
244.365196	7413.804455	8.900647	-0.050301	4.641029
244.163540	7421.764565	8.905651	-0.050269	4.643444
244.074624	7429.789784	8.910656	-0.050257	4.645878
244.484434	7437.855525	8.915661	-0.050339	4.648322
244.592577	7445.807303	8.920666	-0.050364	4.650731
244.824916	7453.873994	8.925671	-0.050413	4.653173
244.754301	7461.880063	8.930675	-0.050405	4.655595
245.135659	7469.871171	8.935680	-0.050481	4.658012
245.218488	7477.869641	8.940685	-0.050502	4.660430
245.373887	7485.890152	8.945690	-0.050536	4.662853
245.510993	7493.912762	8.950695	-0.050567	4.665275
245.546038	7501.925724	8.955699	-0.050578	4.667693
245.835431	7509.949152	8.960704	-0.050638	4.670113
245.723909	7518.055821	8.965709	-0.050622	4.672557
246.018576	7526.091947	8.970714	-0.050682	4.674978
246.133063	7534.065106	8.975719	-0.050709	4.677379
246.137653	7541.976491	8.980723	-0.050715	4.679761
246.487146	7550.097198	8.985728	-0.050785	4.682204
246.454383	7558.007277	8.990733	-0.050784	4.684582
246.534853	7566.050861	8.995738	-0.050804	4.687000
246.974995	7574.088296	9.000743	-0.050892	4.689413
246.897981	7582.073834	9.005747	-0.050882	4.691811
247.037032	7590.116834	9.010752	-0.050914	4.694224
247.232134	7598.178977	9.015757	-0.050955	4.696642
247.508986	7606.110482	9.020762	-0.051012	4.699019
247.774944	7614.123169	9.025767	-0.051067	4.701419
247.796761	7622.127898	9.030771	-0.051076	4.703816
248.111213	7630.177467	9.035776	-0.051140	4.706225
248.230908	7638.219390	9.040781	-0.051167	4.708630
248.441468	7646.221269	9.045786	-0.051212	4.711023
248.580898	7654.275856	9.050791	-0.051243	4.713429
248.620463	7662.232402	9.055795	-0.051256	4.715806
248.724009	7670.269873	9.060800	-0.051280	4.718205
248.837122	7678.268655	9.065805	-0.051306	4.720591
249.039198	7686.269166	9.070810	-0.051349	4.722977
249.176658	7694.340283	9.075815	-0.051380	4.725382
249.243969	7702.311170	9.080819	-0.051398	4.727757
249.468674	7710.373547	9.085824	-0.051445	4.730157
249.466061	7718.411736	9.090829	-0.051450	4.732550
249.621794	7726.382043	9.095834	-0.051484	4.734920
250.223909	7734.430119	9.100839	-0.051601	4.737311
250.072831	7742.416102	9.105843	-0.051578	4.739685
250.223981	7750.408076	9.110848	-0.051612	4.742058
250.590933	7758.375862	9.115853	-0.051685	4.744423
250.799864	7766.483963	9.120858	-0.051730	4.746828
250.922700	7774.474243	9.125863	-0.051758	4.749197
250.975380	7782.538381	9.130867	-0.051773	4.751587
251.295732	7790.564281	9.135872	-0.051838	4.753964
251.275357	7798.565138	9.140877	-0.051839	4.756333
251.261866	7806.500428	9.145882	-0.051842	4.758682
251.544020	7814.541296	9.150887	-0.051899	4.761060
251.698536	7822.544637	9.155891	-0.051933	4.763426
251.917136	7830.547520	9.160896	-0.051979	4.765790
252.064904	7838.607512	9.165901	-0.052012	4.768170
252.329292	7846.567286	9.170906	-0.052067	4.770519
252.575032	7854.637739	9.175911	-0.052118	4.772900
252.614972	7862.636602	9.180915	-0.052130	4.775259
252.835114	7870.670413	9.185920	-0.052177	4.777626
253.099060	7878.681330	9.190925	-0.052231	4.779985
253.133584	7886.678363	9.195930	-0.052243	4.782340
253.374856	7894.670526	9.200935	-0.052293	4.784692
253.636511	7902.692480	9.205939	-0.052347	4.787051
253.614026	7910.704930	9.210944	-0.052348	4.789407
253.606906	7918.795920	9.215949	-0.052352	4.791785
253.771042	7926.782864	9.220954	-0.052387	4.794131
253.886305	7934.833694	9.225959	-0.052414	4.796494
253.837153	7942.747767	9.230963	-0.052410	4.798817
254.118809	7950.781373	9.235968	-0.052468	4.801172
254.471665	7958.824389	9.240973	-0.052539	4.803528
254.672056	7966.827576	9.245978	-0.052581	4.805873
254.856516	7974.853697	9.250983	-0.052621	4.808223
254.893405	7982.818545	9.255987	-0.052633	4.810554
255.136690	7990.265522	9.260992	-0.052683	4.812732
255.193013	7994.773849	9.265997	-0.052697	4.814050
255.305183	7997.083760	9.271002	-0.052719	4.814725
255.621024	7998.486507	9.276007	-0.052779	4.815134
255.511139	7998.969487	9.281011	-0.052759	4.815276
255.491980	7999.931272	9.286016	-0.052756	4.815557
255.696746	7999.924997	9.291021	-0.052794	4.815554
255.537208	7999.901043	9.296026	-0.052764	4.815548
255.749687	7999.921591	9.301031	-0.052804	4.815553
255.761585	7999.936736	9.306035	-0.052806	4.815557
255.760373	7999.939921	9.311040	-0.052806	4.815558
255.697056	7999.954908	9.316045	-0.052794	4.815563
256.016179	7999.918462	9.321050	-0.052853	4.815551
256.155199	7999.931407	9.326055	-0.052879	4.815554
256.181302	7999.944647	9.331059	-0.052884	4.815558
256.151102	7999.936681	9.336064	-0.052879	4.815556
256.368267	7999.950900	9.341069	-0.052919	4.815559
256.142222	7999.923725	9.346074	-0.052877	4.815552
256.334036	7999.950344	9.351079	-0.052913	4.815559
256.229874	7999.913409	9.356083	-0.052893	4.815548
256.364998	7999.961530	9.361088	-0.052919	4.815562
256.324682	7999.969417	9.366093	-0.052911	4.815564
256.315925	7999.927629	9.371098	-0.052909	4.815552
256.494959	7999.982873	9.376103	-0.052943	4.815567
256.426773	7999.951863	9.381107	-0.052930	4.815559
256.354774	7999.984862	9.386112	-0.052917	4.815569
256.701313	7999.959542	9.391117	-0.052981	4.815560
256.544279	7999.953781	9.396122	-0.052952	4.815559
256.568983	7999.985153	9.401127	-0.052957	4.815568
256.388334	7999.922410	9.406131	-0.052923	4.815550
256.682843	7999.972061	9.411136	-0.052978	4.815563
256.605672	7999.955854	9.416141	-0.052964	4.815559
256.513276	7999.962893	9.421146	-0.052946	4.815562
256.879591	7999.953913	9.426151	-0.053015	4.815557
256.767098	7999.931792	9.431155	-0.052994	4.815551
256.644625	7999.961833	9.436160	-0.052971	4.815561
256.892859	7999.954133	9.441165	-0.053017	4.815557
256.656725	7999.957761	9.446170	-0.052973	4.815559
256.694573	7999.961583	9.451175	-0.052980	4.815560
256.651708	7999.956614	9.456179	-0.052972	4.815559
256.660092	7999.987720	9.461184	-0.052974	4.815568
256.769689	7999.963878	9.466189	-0.052994	4.815561
256.867677	7999.970816	9.471194	-0.053012	4.815562
256.951402	7999.980725	9.476199	-0.053028	4.815565
256.684498	7999.935797	9.481203	-0.052978	4.815553
256.790229	7999.961014	9.486208	-0.052998	4.815560
256.733660	7999.934465	9.491213	-0.052988	4.815552
256.765265	7999.917895	9.496218	-0.052993	4.815547
256.748095	7999.951788	9.501223	-0.052990	4.815557
256.903780	7999.926562	9.506227	-0.053019	4.815549
257.052575	7999.998401	9.511232	-0.053047	4.815569
256.798070	7999.944064	9.516237	-0.053000	4.815555
256.783363	7999.955572	9.521242	-0.052997	4.815558
257.080971	7999.973238	9.526247	-0.053052	4.815562
256.948104	7999.948648	9.531251	-0.053028	4.815555
257.057600	7999.968588	9.536256	-0.053048	4.815561
257.135117	7999.963445	9.541261	-0.053062	4.815559
257.135466	7999.932484	9.546266	-0.053063	4.815550
257.254172	7999.963253	9.551271	-0.053085	4.815558
257.201244	7999.944237	9.556275	-0.053075	4.815553
257.188681	7999.964323	9.561280	-0.053072	4.815559
257.204673	7999.962449	9.566285	-0.053075	4.815558
257.070527	7999.936771	9.571290	-0.053050	4.815551
257.109902	7999.960907	9.576295	-0.053058	4.815558
257.159380	7999.942493	9.581299	-0.053067	4.815552
257.096849	7999.972443	9.586304	-0.053055	4.815562
257.363055	7999.972512	9.591309	-0.053105	4.815560
257.200302	7999.931417	9.596314	-0.053075	4.815549
257.242064	7999.954524	9.601319	-0.053083	4.815556
257.284039	7999.924241	9.606323	-0.053090	4.815547
257.343896	7999.964730	9.611328	-0.053102	4.815558
257.378439	7999.977041	9.616333	-0.053108	4.815562
257.109716	7999.920335	9.621338	-0.053058	4.815546
257.187001	7999.944022	9.626343	-0.053072	4.815553
257.192088	7999.929156	9.631347	-0.053073	4.815548
257.171236	7999.944835	9.636352	-0.053069	4.815553
257.180416	7999.965276	9.641357	-0.053071	4.815559
257.183474	7999.931155	9.646362	-0.053072	4.815549
257.271781	7999.972107	9.651367	-0.053088	4.815561
257.163985	7999.925500	9.656371	-0.053068	4.815547
257.449299	7999.945102	9.661376	-0.053121	4.815552
257.458574	7999.968748	9.666381	-0.053123	4.815559
257.230055	7999.937259	9.671386	-0.053080	4.815551
257.273307	7999.983885	9.676391	-0.053089	4.815564
257.346831	7999.937029	9.681395	-0.053102	4.815550
257.305317	7999.987612	9.686400	-0.053095	4.815565
257.328468	7999.976244	9.691405	-0.053099	4.815562
257.308645	7999.982330	9.696410	-0.053095	4.815563
257.328537	8000.004013	9.701415	-0.053099	4.815570
257.463676	7999.973113	9.706419	-0.053124	4.815560
257.661926	7999.964599	9.711424	-0.053161	4.815557
257.543525	7999.976552	9.716429	-0.053139	4.815561
257.349227	7999.950961	9.721434	-0.053103	4.815554
257.433978	7999.974769	9.726439	-0.053119	4.815561
257.475284	7999.933796	9.731443	-0.053126	4.815548
257.649433	7999.924889	9.736448	-0.053159	4.815545
257.523779	7999.950607	9.741453	-0.053135	4.815553
257.563138	7999.919213	9.746458	-0.053143	4.815544
257.626693	8000.003546	9.751463	-0.053155	4.815568
257.547605	7999.965950	9.756467	-0.053140	4.815557
257.526514	7999.975218	9.761472	-0.053136	4.815560
257.464955	7999.966741	9.766477	-0.053124	4.815558
257.397514	7999.932538	9.771482	-0.053112	4.815548
257.824336	7999.986485	9.776487	-0.053191	4.815562
257.884754	7999.971453	9.781491	-0.053203	4.815557
257.720164	8000.006147	9.786496	-0.053172	4.815568
257.522831	7999.964486	9.791501	-0.053135	4.815557
257.761200	7999.953423	9.796506	-0.053180	4.815553
257.804781	7999.950931	9.801511	-0.053188	4.815552
257.622931	7999.931949	9.806515	-0.053154	4.815547
257.631505	7999.953448	9.811520	-0.053156	4.815553
257.804199	7999.986166	9.816525	-0.053188	4.815562
257.590666	7999.947445	9.821530	-0.053148	4.815552
257.675477	7999.984070	9.826535	-0.053164	4.815562
257.814002	7999.958564	9.831539	-0.053190	4.815554
257.729028	7999.948637	9.836544	-0.053174	4.815552
257.662260	7999.976383	9.841549	-0.053161	4.815560
257.722132	7999.952798	9.846554	-0.053173	4.815553
257.849161	7999.955939	9.851559	-0.053196	4.815553
257.549043	7999.946775	9.856563	-0.053140	4.815552
257.789991	7999.962452	9.861568	-0.053185	4.815555
258.027376	7999.993021	9.866573	-0.053230	4.815563
257.828648	7999.975899	9.871578	-0.053193	4.815559
257.608898	7999.976589	9.876583	-0.053152	4.815560
257.756080	7999.933070	9.881587	-0.053179	4.815547
257.860729	7999.975358	9.886592	-0.053199	4.815559
257.898936	7999.981322	9.891597	-0.053206	4.815560
257.668094	7999.985034	9.896602	-0.053163	4.815562
257.875989	7999.975610	9.901607	-0.053201	4.815559
257.830890	7999.957790	9.906611	-0.053193	4.815554
257.877970	7999.951083	9.911616	-0.053202	4.815552
257.906615	7999.994268	9.916621	-0.053207	4.815564
257.657715	7999.954970	9.921626	-0.053161	4.815554
257.636650	7999.964239	9.926631	-0.053157	4.815557
257.904027	7999.973939	9.931635	-0.053207	4.815558
257.945295	7999.988496	9.936640	-0.053214	4.815562
257.796333	7999.966846	9.941645	-0.053187	4.815557
257.967911	7999.944015	9.946650	-0.053219	4.815549
257.952935	7999.995031	9.951655	-0.053216	4.815564
257.891627	7999.937434	9.956659	-0.053204	4.815547
257.745263	7999.952135	9.961664	-0.053177	4.815552
258.056407	7999.957210	9.966669	-0.053235	4.815552
257.831320	7999.940726	9.971674	-0.053193	4.815549
257.780761	7999.970872	9.976679	-0.053184	4.815558
257.831812	7999.945008	9.981683	-0.053193	4.815550
257.833643	7999.977076	9.986688	-0.053194	4.815559
257.580069	7999.985758	9.991693	-0.053147	4.815563
257.714493	7999.971932	9.996698	-0.053172	4.815558
258.024818	7999.986605	10.001703	-0.053229	4.815561
257.871563	7999.941391	10.006707	-0.053201	4.815549
257.777794	7999.981511	10.011712	-0.053183	4.815561
257.938033	7999.972378	10.016717	-0.053213	4.815557
258.001243	7999.953120	10.021722	-0.053225	4.815552
258.130997	7999.993682	10.026727	-0.053249	4.815563
257.993295	7999.973283	10.031731	-0.053224	4.815557
257.980841	7999.962402	10.036736	-0.053221	4.815554
258.083170	7999.986498	10.041741	-0.053240	4.815561
258.132818	7999.987309	10.046746	-0.053250	4.815561
258.192413	7999.997893	10.051751	-0.053261	4.815564
257.836720	7999.968600	10.056755	-0.053195	4.815557
257.856731	7999.993489	10.061760	-0.053198	4.815564
258.045480	7999.975210	10.066765	-0.053233	4.815558
258.235318	7999.967628	10.071770	-0.053269	4.815555
258.079069	7999.999254	10.076775	-0.053240	4.815565
258.001845	7999.968095	10.081779	-0.053225	4.815556
258.088827	7999.983397	10.086784	-0.053242	4.815560
258.206871	7999.986391	10.091789	-0.053264	4.815560
258.085104	7999.979067	10.096794	-0.053241	4.815559
258.117230	8000.015901	10.101799	-0.053247	4.815569
258.111651	7999.994453	10.106803	-0.053246	4.815563
258.128230	7999.989385	10.111808	-0.053249	4.815562
258.111375	8000.000859	10.116813	-0.053246	4.815565
257.884953	7999.991828	10.121818	-0.053204	4.815563
257.947526	8000.019547	10.126823	-0.053215	4.815571
258.165466	7999.977183	10.131827	-0.053256	4.815558
258.123484	7999.981839	10.136832	-0.053248	4.815559
258.266104	8000.021543	10.141837	-0.053275	4.815570
258.147328	7999.975822	10.146842	-0.053253	4.815557
258.318705	8000.018131	10.151847	-0.053285	4.815569
258.217645	7999.992990	10.156851	-0.053266	4.815562
258.108544	7999.982669	10.161856	-0.053245	4.815560
258.159355	8000.010197	10.166861	-0.053255	4.815567
258.074175	7999.984247	10.171866	-0.053239	4.815560
258.168338	7999.998598	10.176871	-0.053257	4.815564
258.148316	7999.971575	10.181875	-0.053253	4.815556
258.148377	7999.970510	10.186880	-0.053253	4.815556
258.166281	8000.006044	10.191885	-0.053256	4.815566
258.100172	7999.980405	10.196890	-0.053244	4.815559
258.120034	8000.010632	10.201895	-0.053248	4.815568
258.267309	8000.007695	10.206899	-0.053275	4.815566
258.178230	8000.003040	10.211904	-0.053259	4.815565
258.159705	8000.004875	10.216909	-0.053255	4.815566
258.074383	7999.982126	10.221914	-0.053239	4.815560
258.191708	8000.018214	10.226919	-0.053261	4.815570
258.017387	7999.966249	10.231923	-0.053229	4.815555
258.033308	7999.984664	10.236928	-0.053232	4.815561
258.149727	8000.002582	10.241933	-0.053253	4.815565
258.141176	7999.999240	10.246938	-0.053252	4.815564
258.135447	7999.983130	10.251943	-0.053251	4.815560
258.132821	7999.971341	10.256947	-0.053250	4.815556
258.082583	7999.999356	10.261952	-0.053241	4.815565
258.139012	8000.008821	10.266957	-0.053251	4.815567
258.311141	7999.993475	10.271962	-0.053283	4.815562
258.433118	8000.017892	10.276967	-0.053306	4.815568
258.324667	7999.986223	10.281971	-0.053286	4.815560
258.236811	7999.983723	10.286976	-0.053270	4.815559
258.274816	8000.017449	10.291981	-0.053277	4.815569
257.984589	7999.944372	10.296986	-0.053223	4.815549
258.240769	7999.994470	10.301991	-0.053270	4.815562
258.214071	7999.973746	10.306995	-0.053265	4.815557
258.077133	7999.974718	10.312000	-0.053240	4.815557
258.173415	7999.990172	10.317005	-0.053258	4.815562
258.396623	7999.969251	10.322010	-0.053300	4.815554
258.392417	7999.981999	10.327015	-0.053299	4.815558
258.281924	7999.965247	10.332019	-0.053278	4.815554
258.271760	7999.973626	10.337024	-0.053276	4.815556
258.288092	7999.986708	10.342029	-0.053279	4.815560
258.151241	7999.970595	10.347034	-0.053254	4.815556
258.214948	7999.988722	10.352039	-0.053266	4.815561
258.469140	7999.970442	10.357043	-0.053313	4.815554
258.315590	7999.994637	10.362048	-0.053285	4.815562
258.383826	8000.006430	10.367053	-0.053297	4.815565
258.192567	7999.958460	10.372058	-0.053262	4.815552
258.263045	8000.003395	10.377063	-0.053275	4.815565
258.226071	8000.014540	10.382067	-0.053268	4.815568
258.488257	7999.987848	10.387072	-0.053317	4.815559
258.384286	8000.016055	10.392077	-0.053297	4.815568
258.194685	7999.980927	10.397082	-0.053262	4.815559
258.224958	7999.985693	10.402087	-0.053268	4.815560
258.452440	8000.001152	10.407091	-0.053310	4.815563
258.415058	7999.994136	10.412096	-0.053303	4.815562
258.372732	8000.022280	10.417101	-0.053295	4.815570
258.425254	7999.995372	10.422106	-0.053305	4.815562
258.427683	8000.050945	10.427111	-0.053306	4.815578
258.448308	8000.027788	10.432115	-0.053309	4.815571
258.505639	8000.034064	10.437120	-0.053320	4.815573
258.421117	8000.022008	10.442125	-0.053304	4.815570
258.145519	7999.990816	10.447130	-0.053253	4.815562
258.342599	8000.002575	10.452135	-0.053290	4.815564
258.467326	7999.989659	10.457139	-0.053313	4.815560
258.326081	7999.986289	10.462144	-0.053287	4.815560
258.196299	8000.008736	10.467149	-0.053263	4.815567
258.278655	7999.975907	10.472154	-0.053278	4.815557
258.407439	8000.016453	10.477159	-0.053302	4.815568
258.240442	7999.997712	10.482163	-0.053271	4.815563
258.288619	7999.984616	10.487168	-0.053280	4.815559
258.384466	8000.019286	10.492173	-0.053298	4.815569
258.306977	7999.981714	10.497178	-0.053283	4.815558
258.418415	8000.015571	10.502183	-0.053304	4.815568
258.396403	7999.981039	10.507187	-0.053300	4.815558
258.272702	7999.950190	10.512192	-0.053277	4.815549
258.352446	8000.019838	10.517197	-0.053292	4.815569
258.420427	7999.992114	10.522202	-0.053305	4.815561
258.353031	8000.019850	10.527207	-0.053292	4.815569
258.387053	7999.993708	10.532211	-0.053298	4.815562
258.418928	7999.997433	10.537216	-0.053304	4.815562
258.692098	8000.021112	10.542221	-0.053355	4.815568
258.575710	7999.974362	10.547226	-0.053333	4.815555
258.311223	8000.002087	10.552231	-0.053284	4.815564
258.436527	7999.989181	10.557235	-0.053308	4.815560
258.315944	7999.980808	10.562240	-0.053285	4.815558
258.280874	8000.016547	10.567245	-0.053279	4.815569
258.123746	7999.970201	10.572250	-0.053249	4.815556
258.154551	7999.995267	10.577255	-0.053255	4.815563
258.165254	7999.984763	10.582259	-0.053257	4.815560
258.094748	7999.980411	10.587264	-0.053244	4.815559
258.374632	8000.009539	10.592269	-0.053296	4.815566
258.176629	7999.972138	10.597274	-0.053259	4.815556
258.165953	7999.984780	10.602279	-0.053257	4.815560
258.489844	8000.000742	10.607283	-0.053318	4.815563
258.311137	8000.004236	10.612288	-0.053284	4.815565
258.468102	8000.010001	10.617293	-0.053314	4.815566
258.495122	7999.978406	10.622298	-0.053319	4.815557
258.692471	8000.017935	10.627303	-0.053355	4.815567
258.395041	7999.989591	10.632307	-0.053300	4.815560
258.247036	7999.971160	10.637312	-0.053273	4.815556
258.413728	8000.027275	10.642317	-0.053304	4.815571
258.389373	7999.995909	10.647322	-0.053299	4.815562
258.405260	8000.031411	10.652327	-0.053302	4.815572
258.402802	8000.008946	10.657331	-0.053302	4.815566
258.578721	7999.988322	10.662336	-0.053334	4.815559
258.642029	8000.016054	10.667341	-0.053346	4.815567
258.558907	7999.993341	10.672346	-0.053331	4.815561
258.613457	8000.008115	10.677351	-0.053341	4.815565
258.509620	7999.997879	10.682355	-0.053322	4.815562
258.601594	8000.001516	10.687360	-0.053339	4.815563
258.769150	8000.012794	10.692365	-0.053370	4.815565
258.745083	8000.011335	10.697370	-0.053365	4.815565
258.715530	8000.020465	10.702375	-0.053360	4.815568
258.347488	8000.031550	10.707379	-0.053291	4.815573
258.548568	8000.038035	10.712384	-0.053329	4.815574
258.500104	8000.038313	10.717389	-0.053320	4.815574
258.494959	7999.975223	10.722394	-0.053319	4.815556
258.708834	8000.016090	10.727399	-0.053359	4.815567
258.649959	8000.004452	10.732403	-0.053348	4.815563
258.427126	7999.995479	10.737408	-0.053306	4.815562
258.559054	8000.013651	10.742413	-0.053331	4.815567
258.565087	7999.975305	10.747418	-0.053332	4.815555
258.550889	8000.028471	10.752423	-0.053329	4.815571
258.555212	8000.007184	10.757427	-0.053330	4.815565
258.455496	8000.032257	10.762432	-0.053312	4.815572
258.489426	8000.032812	10.767437	-0.053318	4.815572
258.522026	8000.001307	10.772442	-0.053324	4.815563
258.592470	8000.025952	10.777447	-0.053337	4.815570
258.688347	7999.984800	10.782451	-0.053355	4.815557
258.386003	8000.005500	10.787456	-0.053299	4.815565
258.587603	8000.005585	10.792461	-0.053336	4.815564
258.651326	8000.004490	10.797466	-0.053348	4.815563
258.491241	8000.024306	10.802471	-0.053318	4.815570
258.479696	8000.023051	10.807475	-0.053316	4.815570
258.514378	7999.988377	10.812480	-0.053323	4.815559
258.532664	8000.019646	10.817485	-0.053326	4.815568
258.351730	7999.985727	10.822490	-0.053293	4.815559
258.611862	8000.014533	10.827495	-0.053341	4.815567
258.673672	8000.043308	10.832499	-0.053353	4.815575
258.408740	8000.033649	10.837504	-0.053303	4.815573
258.520714	8000.056835	10.842509	-0.053324	4.815579
258.570541	8000.021339	10.847514	-0.053333	4.815569
258.543323	7999.984587	10.852519	-0.053328	4.815558
258.605904	8000.002696	10.857523	-0.053340	4.815563
258.539005	7999.993062	10.862528	-0.053328	4.815561
258.712923	8000.012987	10.867533	-0.053360	4.815566
258.576097	7999.996874	10.872538	-0.053334	4.815562
258.836977	8000.028896	10.877543	-0.053383	4.815570
258.718815	8000.017359	10.882547	-0.053361	4.815567
258.596813	8000.010030	10.887552	-0.053338	4.815565
258.658792	8000.035605	10.892557	-0.053350	4.815572
258.847361	8000.001304	10.897562	-0.053385	4.815562
258.830543	8000.039477	10.902567	-0.053382	4.815573
258.712819	8000.015131	10.907571	-0.053360	4.815566
258.704444	7999.998977	10.912576	-0.053358	4.815562
258.700643	8000.030954	10.917581	-0.053358	4.815571
258.537373	7999.995186	10.922586	-0.053327	4.815561
258.726852	8000.015365	10.927591	-0.053363	4.815566
258.886376	8000.030783	10.932595	-0.053392	4.815570
258.882096	8000.042462	10.937600	-0.053392	4.815573
258.820478	8000.051069	10.942605	-0.053380	4.815576
258.863545	7999.985562	10.947610	-0.053388	4.815557
258.863307	8000.040023	10.952615	-0.053388	4.815573
258.728790	8000.007928	10.957619	-0.053363	4.815564
258.651761	7999.995994	10.962624	-0.053349	4.815561
258.637297	8000.020321	10.967629	-0.053346	4.815568
258.650782	7999.986369	10.972634	-0.053349	4.815558
258.822903	8000.018012	10.977639	-0.053381	4.815567
258.934480	8000.019833	10.982643	-0.053402	4.815567
258.782849	7999.974644	10.987648	-0.053373	4.815554
258.719820	8000.012062	10.992653	-0.053362	4.815565
258.929744	8000.006944	10.997658	-0.053401	4.815563
258.992594	8000.007971	11.002663	-0.053412	4.815563
258.847999	8000.010953	11.007667	-0.053385	4.815564
258.820864	7999.995560	11.012672	-0.053380	4.815560
258.767393	8000.019252	11.017677	-0.053371	4.815567
258.819798	7999.995545	11.022682	-0.053380	4.815560
258.792435	8000.022866	11.027687	-0.053375	4.815568
258.928206	8000.043237	11.032691	-0.053401	4.815573
258.726450	7999.985483	11.037696	-0.053363	4.815557
258.783859	7999.999236	11.042701	-0.053374	4.815561
258.695127	7999.970023	11.047706	-0.053357	4.815553
258.779130	8000.005568	11.052711	-0.053373	4.815563
258.667113	7999.997335	11.057715	-0.053352	4.815561
258.690372	7999.992376	11.062720	-0.053356	4.815560
258.888900	8000.039401	11.067725	-0.053393	4.815572
258.830403	8000.009613	11.072730	-0.053382	4.815564
258.598854	8000.028264	11.077735	-0.053339	4.815571
258.862080	8000.011201	11.082739	-0.053388	4.815564
258.761211	8000.006353	11.087744	-0.053370	4.815563
258.849054	8000.030213	11.092749	-0.053386	4.815570
258.908779	7999.988472	11.097754	-0.053397	4.815557
258.877131	8000.034945	11.102759	-0.053391	4.815571
258.870358	8000.047651	11.107763	-0.053390	4.815575
258.553242	8000.022189	11.112768	-0.053331	4.815569
258.823092	8000.058630	11.117773	-0.053381	4.815578
258.734027	8000.004850	11.122778	-0.053365	4.815563
258.735136	8000.041179	11.127783	-0.053365	4.815574
258.996595	7999.997388	11.132787	-0.053413	4.815560
258.750619	7999.976290	11.137792	-0.053368	4.815555
258.793403	8000.006891	11.142797	-0.053376	4.815563
258.873251	8000.001787	11.147802	-0.053391	4.815562
258.877604	8000.024286	11.152807	-0.053391	4.815568
258.865693	8000.008074	11.157811	-0.053389	4.815563
258.610506	7999.968671	11.162816	-0.053342	4.815553
258.825606	8000.004219	11.167821	-0.053382	4.815562
258.782262	8000.001377	11.172826	-0.053374	4.815562
258.711460	7999.991680	11.177831	-0.053361	4.815559
258.744940	7999.985820	11.182835	-0.053367	4.815557
258.905010	7999.979888	11.187840	-0.053397	4.815555
258.936425	8000.025255	11.192845	-0.053402	4.815568
259.044671	8000.005664	11.197850	-0.053423	4.815562
259.085988	7999.991388	11.202855	-0.053430	4.815557
258.909350	8000.017342	11.207859	-0.053397	4.815566
258.789152	7999.988684	11.212864	-0.053375	4.815558
258.985693	8000.034608	11.217869	-0.053412	4.815571
258.867639	7999.969676	11.222874	-0.053390	4.815552
258.663222	7999.998381	11.227879	-0.053352	4.815562
258.895986	8000.009654	11.232883	-0.053395	4.815564
258.978476	7999.983235	11.237888	-0.053410	4.815556
258.985348	8000.027133	11.242893	-0.053412	4.815568
258.792775	7999.980208	11.247898	-0.053376	4.815556
258.764734	7999.976548	11.252903	-0.053371	4.815555
258.846869	7999.991772	11.257907	-0.053386	4.815559
258.670019	7999.973938	11.262912	-0.053353	4.815554
258.912239	8000.015267	11.267917	-0.053398	4.815565
258.946120	7999.977376	11.272922	-0.053404	4.815554
259.018626	8000.004190	11.277927	-0.053418	4.815562
258.970020	8000.007670	11.282931	-0.053409	4.815563
258.921276	7999.998333	11.287936	-0.053400	4.815560
258.881603	8000.009434	11.292941	-0.053393	4.815564
258.970187	8000.001269	11.297946	-0.053409	4.815561
258.993697	7999.999518	11.302951	-0.053413	4.815560
259.015318	8000.013755	11.307955	-0.053417	4.815564
258.909348	8000.006688	11.312960	-0.053398	4.815563
259.031187	8000.018288	11.317965	-0.053420	4.815566
258.982749	7999.973714	11.322970	-0.053411	4.815553
258.961395	7999.953076	11.327975	-0.053407	4.815547
259.022495	7999.997859	11.332979	-0.053419	4.815560
259.126193	7999.974989	11.337984	-0.053438	4.815552
259.206121	8000.022216	11.342989	-0.053453	4.815566
259.032893	7999.979877	11.347994	-0.053421	4.815554
259.070385	7999.995441	11.352999	-0.053428	4.815559
259.220239	8000.026722	11.358003	-0.053456	4.815567
258.912341	8000.009952	11.363008	-0.053398	4.815564
259.128170	8000.024154	11.368013	-0.053439	4.815567
259.197277	8000.003924	11.373018	-0.053452	4.815561
259.121651	8000.002691	11.378023	-0.053437	4.815561
258.795516	8000.009120	11.383027	-0.053377	4.815564
258.909144	7999.978936	11.388032	-0.053398	4.815555
259.135265	8000.039227	11.393037	-0.053440	4.815571
258.839548	8000.007706	11.398042	-0.053385	4.815563
258.834911	8000.008699	11.403047	-0.053384	4.815564
259.005330	8000.010412	11.408051	-0.053416	4.815563
258.830699	7999.994750	11.413056	-0.053383	4.815560
258.923238	8000.009076	11.418061	-0.053401	4.815563
258.951374	7999.973226	11.423066	-0.053406	4.815553
259.106669	7999.999255	11.428071	-0.053435	4.815560
259.148398	8000.017024	11.433075	-0.053443	4.815565
259.018641	7999.987142	11.438080	-0.053418	4.815557
259.243198	8000.030321	11.443085	-0.053460	4.815568
259.266970	7999.998672	11.448090	-0.053465	4.815559
259.049518	8000.009008	11.453095	-0.053424	4.815563
259.303894	8000.035586	11.458099	-0.053472	4.815569
259.097010	7999.983087	11.463104	-0.053433	4.815555
259.009241	8000.038257	11.468109	-0.053417	4.815572
259.183517	8000.015471	11.473114	-0.053449	4.815564
259.198061	8000.015710	11.478119	-0.053452	4.815564
259.240942	7999.996120	11.483123	-0.053460	4.815558
259.118113	7999.978098	11.488128	-0.053437	4.815553
259.398061	8000.026452	11.493133	-0.053489	4.815566
259.170886	8000.000320	11.498138	-0.053447	4.815560
259.099280	8000.025851	11.503143	-0.053434	4.815567
259.359624	8000.038644	11.508147	-0.053482	4.815570
259.022453	8000.002174	11.513152	-0.053419	4.815561
259.203998	8000.028631	11.518157	-0.053453	4.815568
259.338482	8000.012672	11.523162	-0.053478	4.815562
259.160864	8000.011911	11.528167	-0.053445	4.815563
259.077158	8000.021226	11.533171	-0.053430	4.815566
259.185318	7999.996293	11.538176	-0.053450	4.815558
259.198380	8000.023206	11.543181	-0.053452	4.815566
259.016376	8000.010626	11.548186	-0.053418	4.815563
259.204155	8000.014759	11.553191	-0.053453	4.815564
259.296002	8000.039754	11.558195	-0.053470	4.815571
259.278522	8000.020247	11.563200	-0.053467	4.815565
259.220309	8000.043861	11.568205	-0.053456	4.815572
259.229700	8000.011977	11.573210	-0.053458	4.815563
259.346115	8000.038440	11.578215	-0.053480	4.815570
259.435840	8000.040973	11.583219	-0.053497	4.815570
259.190144	8000.007063	11.588224	-0.053451	4.815562
259.422821	8000.020472	11.593229	-0.053494	4.815564
259.264661	8000.029640	11.598234	-0.053465	4.815568
259.315038	8000.031532	11.603239	-0.053474	4.815568
259.418823	8000.036430	11.608243	-0.053493	4.815569
259.265089	8000.015768	11.613248	-0.053465	4.815564
259.270707	8000.028676	11.618253	-0.053466	4.815567
259.215773	8000.013898	11.623258	-0.053456	4.815563
259.245155	8000.003699	11.628263	-0.053461	4.815560
259.207979	8000.020181	11.633267	-0.053454	4.815565
259.106710	8000.039888	11.638272	-0.053435	4.815572
259.166409	8000.050475	11.643277	-0.053447	4.815574
259.115532	8000.014404	11.648282	-0.053437	4.815564
259.162829	7999.975663	11.653287	-0.053446	4.815552
259.318016	8000.010235	11.658291	-0.053475	4.815562
259.230878	7999.967165	11.663296	-0.053459	4.815550
259.420143	8000.010835	11.668301	-0.053494	4.815562
259.328406	7999.994389	11.673306	-0.053477	4.815557
259.291567	8000.019419	11.678311	-0.053470	4.815565
259.459920	8000.042459	11.683315	-0.053501	4.815571
259.383167	7999.973927	11.688320	-0.053487	4.815551
259.329169	8000.006153	11.693325	-0.053477	4.815561
259.346792	8000.009646	11.698330	-0.053480	4.815562
259.257050	8000.029542	11.703335	-0.053464	4.815568
259.309586	8000.028264	11.708339	-0.053473	4.815567
259.268462	8000.020119	11.713344	-0.053466	4.815565
259.329086	8000.028585	11.718349	-0.053477	4.815567
259.198218	8000.001888	11.723354	-0.053453	4.815560
259.422771	8000.038659	11.728359	-0.053495	4.815570
259.444200	8000.055029	11.733363	-0.053499	4.815574
259.303236	8000.031372	11.738368	-0.053472	4.815568
259.417091	8000.055658	11.743373	-0.053494	4.815575
259.264473	8000.008315	11.748378	-0.053465	4.815562
259.060052	8000.023136	11.753383	-0.053427	4.815567
259.415933	8000.031080	11.758387	-0.053493	4.815567
259.436086	8000.015390	11.763392	-0.053497	4.815563
259.393353	8000.055276	11.768397	-0.053489	4.815575
259.469144	8000.019136	11.773402	-0.053503	4.815564
259.375465	8000.003725	11.778407	-0.053486	4.815560
259.347746	8000.050264	11.783411	-0.053481	4.815573
259.377195	8000.028319	11.788416	-0.053486	4.815567
259.465348	8000.023351	11.793421	-0.053503	4.815565
259.470251	8000.015956	11.798426	-0.053504	4.815563
259.374499	8000.016531	11.803431	-0.053486	4.815563
259.566313	8000.035681	11.808435	-0.053521	4.815568
259.439824	8000.015463	11.813440	-0.053498	4.815563
259.206089	8000.022330	11.818445	-0.053454	4.815566
259.084162	8000.008595	11.823450	-0.053432	4.815562
259.198530	7999.991239	11.828455	-0.053453	4.815557
259.282892	8000.013976	11.833459	-0.053469	4.815563
259.067229	7999.992304	11.838464	-0.053429	4.815558
259.496210	8000.013187	11.843469	-0.053508	4.815562
259.436321	8000.006871	11.848474	-0.053497	4.815560
259.366271	7999.999322	11.853479	-0.053484	4.815558
259.289261	8000.034377	11.858483	-0.053470	4.815569
259.443067	8000.006985	11.863488	-0.053499	4.815560
259.327319	8000.031796	11.868493	-0.053477	4.815568
259.381595	8000.027343	11.873498	-0.053487	4.815567
259.516042	8000.022063	11.878503	-0.053512	4.815564
259.507098	8000.041141	11.883507	-0.053511	4.815570
259.298228	7999.995016	11.888512	-0.053472	4.815557
259.424052	8000.028041	11.893517	-0.053495	4.815567
259.404528	8000.008501	11.898522	-0.053492	4.815561
259.198225	7999.999796	11.903527	-0.053453	4.815559
259.316972	8000.033773	11.908531	-0.053475	4.815569
259.341953	8000.023502	11.913536	-0.053480	4.815566
259.364341	8000.035616	11.918541	-0.053484	4.815569
259.228777	8000.003503	11.923546	-0.053459	4.815560
259.278798	8000.002185	11.928551	-0.053468	4.815560
259.331447	8000.028675	11.933555	-0.053478	4.815567
259.190190	8000.021032	11.938560	-0.053452	4.815566
259.287655	8000.042915	11.943565	-0.053470	4.815572
259.327994	8000.015807	11.948570	-0.053477	4.815563
259.225281	7999.999182	11.953575	-0.053458	4.815559
259.368230	8000.042097	11.958579	-0.053485	4.815571
259.394315	8000.015825	11.963584	-0.053490	4.815563
259.500133	8000.061339	11.968589	-0.053510	4.815576
259.275469	8000.036315	11.973594	-0.053468	4.815570
259.300518	8000.036725	11.978599	-0.053472	4.815570
259.384431	8000.045571	11.983603	-0.053488	4.815572
259.363361	8000.033481	11.988608	-0.053484	4.815568
259.427544	8000.058025	11.993613	-0.053496	4.815575
259.628119	8000.036736	11.998618	-0.053533	4.815568
259.435580	8000.047479	12.003623	-0.053498	4.815572
259.426741	8000.036656	12.008627	-0.053496	4.815569
259.228204	8000.039826	12.013632	-0.053459	4.815571
259.526575	8000.048967	12.018637	-0.053515	4.815572
259.424734	8000.037695	12.023642	-0.053496	4.815569
259.362528	8000.019594	12.028647	-0.053484	4.815564
259.525567	8000.056430	12.033651	-0.053515	4.815574
259.447283	8000.028455	12.038656	-0.053500	4.815567
259.394250	8000.054290	12.043661	-0.053490	4.815574
259.363133	8000.016405	12.048666	-0.053484	4.815563
259.397781	8000.021243	12.053671	-0.053491	4.815565
259.304996	8000.042157	12.058675	-0.053473	4.815571
259.295730	8000.018513	12.063680	-0.053472	4.815564
259.333739	8000.036221	12.068685	-0.053479	4.815569
259.422494	8000.016312	12.073690	-0.053495	4.815563
259.466827	8000.030920	12.078695	-0.053504	4.815567
259.503788	8000.063562	12.083699	-0.053511	4.815577
259.310332	8000.014485	12.088704	-0.053475	4.815563
259.454707	8000.016842	12.093709	-0.053501	4.815563
259.423553	8000.019539	12.098714	-0.053496	4.815564
259.467343	8000.002100	12.103719	-0.053504	4.815559
259.446678	8000.039142	12.108723	-0.053500	4.815570
259.361359	8000.015324	12.113728	-0.053484	4.815563
259.349175	8000.024738	12.118733	-0.053482	4.815566
259.341152	8000.020336	12.123738	-0.053480	4.815565
259.483783	8000.019461	12.128743	-0.053507	4.815564
259.670324	8000.048137	12.133747	-0.053542	4.815571
259.406166	7999.989362	12.138752	-0.053493	4.815555
259.411010	8000.014005	12.143757	-0.053493	4.815562
259.456383	8000.023290	12.148762	-0.053502	4.815565
259.458285	8000.020119	12.153767	-0.053502	4.815564
259.626177	8000.010044	12.158771	-0.053534	4.815560
259.603746	7999.997932	12.163776	-0.053529	4.815557
259.614817	8000.032288	12.168781	-0.053531	4.815567
259.506673	8000.032661	12.173786	-0.053511	4.815567
259.632089	8000.017621	12.178791	-0.053535	4.815562
259.716058	8000.040352	12.183795	-0.053550	4.815569
259.721511	8000.010539	12.188800	-0.053551	4.815560
259.390900	8000.030776	12.193805	-0.053490	4.815567
259.625003	8000.033530	12.198810	-0.053533	4.815567
259.375075	8000.011298	12.203815	-0.053487	4.815562
259.549707	8000.044051	12.208819	-0.053519	4.815571
259.633598	8000.029402	12.213824	-0.053535	4.815566
259.650129	8000.045692	12.218829	-0.053538	4.815571
259.634890	8000.036901	12.223834	-0.053535	4.815568
259.564346	8000.035751	12.228839	-0.053522	4.815568
259.732074	8000.027810	12.233843	-0.053553	4.815565
259.655310	8000.014811	12.238848	-0.053539	4.815562
259.584022	8000.024328	12.243853	-0.053526	4.815565
259.577036	8000.023148	12.248858	-0.053525	4.815564
259.609625	8000.024749	12.253863	-0.053531	4.815565
259.790743	8000.060812	12.258867	-0.053565	4.815574
259.684890	8000.035591	12.263872	-0.053545	4.815567
259.586009	8000.046794	12.268877	-0.053526	4.815571
259.655120	8000.062874	12.273882	-0.053539	4.815576
259.579513	8000.033875	12.278887	-0.053525	4.815567
259.758442	8000.066699	12.283891	-0.053559	4.815576
259.673995	8000.025807	12.288896	-0.053543	4.815565
259.542080	8000.058898	12.293901	-0.053518	4.815575
259.558779	8000.027134	12.298906	-0.053521	4.815566
259.753508	8000.014293	12.303911	-0.053558	4.815561
259.783459	8000.043618	12.308915	-0.053563	4.815569
259.689398	8000.010046	12.313920	-0.053546	4.815560
259.655784	8000.034061	12.318925	-0.053540	4.815567
259.760157	8000.035766	12.323930	-0.053559	4.815567
259.535355	8000.035302	12.328935	-0.053517	4.815568
259.629754	8000.034708	12.333939	-0.053535	4.815567
259.539196	8000.010804	12.338944	-0.053518	4.815561
259.677186	8000.048300	12.343949	-0.053544	4.815571
259.608473	8000.018345	12.348954	-0.053531	4.815563
259.657293	8000.023415	12.353959	-0.053540	4.815564
259.645498	8000.056330	12.358963	-0.053538	4.815574
259.576922	8000.016766	12.363968	-0.053525	4.815562
259.720377	8000.050079	12.368973	-0.053552	4.815572
259.777569	8000.065965	12.373978	-0.053562	4.815576
259.431079	8000.034681	12.378983	-0.053498	4.815568
259.779980	8000.060667	12.383987	-0.053563	4.815574
259.722542	8000.042643	12.388992	-0.053552	4.815569
259.655284	8000.038343	12.393997	-0.053540	4.815568
259.491675	8000.047422	12.399002	-0.053509	4.815572
259.471025	8000.027863	12.404007	-0.053505	4.815566
259.407666	8000.047121	12.409011	-0.053494	4.815572
259.389097	8000.009441	12.414016	-0.053490	4.815561
259.714590	8000.031841	12.419021	-0.053551	4.815566
259.645865	8000.034993	12.424026	-0.053538	4.815567
259.485533	8000.020630	12.429031	-0.053508	4.815564
259.491877	8000.035686	12.434035	-0.053509	4.815568
259.644123	8000.034968	12.439040	-0.053538	4.815567
259.538718	8000.068491	12.444045	-0.053518	4.815578
259.541346	8000.015138	12.449050	-0.053519	4.815562
259.493938	8000.013298	12.454055	-0.053510	4.815562
259.519731	8000.040418	12.459059	-0.053515	4.815570
259.495309	8000.020798	12.464064	-0.053510	4.815564
259.638550	8000.040224	12.469069	-0.053537	4.815569
259.613177	8000.045151	12.474074	-0.053532	4.815571
259.589466	8000.039425	12.479079	-0.053528	4.815569
259.511153	8000.027469	12.484083	-0.053513	4.815566
259.656752	7999.994604	12.489088	-0.053540	4.815556
259.493045	8000.031448	12.494093	-0.053510	4.815567
259.539110	8000.022589	12.499098	-0.053518	4.815564
259.724390	8000.037361	12.504103	-0.053553	4.815568
259.904281	8000.079813	12.509107	-0.053586	4.815579
259.505150	8000.028446	12.514112	-0.053512	4.815566
259.621738	8000.035690	12.519117	-0.053534	4.815568
259.546718	8000.040875	12.524122	-0.053520	4.815570
259.516951	8000.006216	12.529127	-0.053514	4.815560
259.634093	8000.034827	12.534131	-0.053536	4.815567
259.657892	7999.995703	12.539136	-0.053540	4.815556
259.606079	8000.017285	12.544141	-0.053531	4.815562
259.755895	8000.036819	12.549146	-0.053559	4.815567
259.683042	8000.014272	12.554151	-0.053545	4.815561
259.688383	8000.023972	12.559155	-0.053546	4.815564
259.523232	8000.002055	12.564160	-0.053515	4.815558
259.515036	8000.024349	12.569165	-0.053514	4.815565
259.736913	8000.032243	12.574170	-0.053555	4.815566
259.724859	8000.004281	12.579175	-0.053553	4.815558
259.805640	8000.024823	12.584179	-0.053568	4.815564
259.689416	8000.020792	12.589184	-0.053547	4.815563
259.751511	8000.050641	12.594189	-0.053558	4.815572
259.948837	8000.044251	12.599194	-0.053595	4.815569
259.813980	8000.042052	12.604199	-0.053570	4.815569
259.991861	8000.067383	12.609203	-0.053603	4.815575
259.839774	8000.032863	12.614208	-0.053575	4.815566
259.788669	8000.046982	12.619213	-0.053565	4.815570
259.760627	8000.058273	12.624218	-0.053560	4.815574
259.789946	8000.043801	12.629223	-0.053565	4.815569
259.822902	8000.045408	12.634227	-0.053572	4.815570
259.922451	8000.010724	12.639232	-0.053590	4.815559
259.942694	8000.044162	12.644237	-0.053594	4.815569
259.860987	8000.051373	12.649242	-0.053579	4.815571
259.833634	8000.038113	12.654247	-0.053574	4.815567
259.973185	8000.078838	12.659251	-0.053600	4.815579
259.672936	8000.024813	12.664256	-0.053544	4.815564
259.691316	8000.059289	12.669261	-0.053547	4.815574
259.929094	8000.052491	12.674266	-0.053591	4.815571
259.903863	8000.054216	12.679271	-0.053587	4.815572
259.788864	8000.059816	12.684275	-0.053565	4.815574
259.722706	8000.010680	12.689280	-0.053553	4.815560
259.654408	8000.026654	12.694285	-0.053540	4.815565
259.713609	8000.014806	12.699290	-0.053551	4.815561
259.489593	8000.021831	12.704295	-0.053510	4.815564
259.761543	8000.049765	12.709299	-0.053560	4.815571
259.719236	8000.005290	12.714304	-0.053552	4.815558
259.606156	8000.016261	12.719309	-0.053531	4.815562
259.687513	8000.029337	12.724314	-0.053547	4.815566
259.588171	8000.022378	12.729319	-0.053528	4.815564
259.770577	8000.057394	12.734323	-0.053562	4.815573
259.966893	8000.047784	12.739328	-0.053599	4.815570
259.828484	8000.049798	12.744333	-0.053573	4.815571
259.640395	8000.039254	12.749338	-0.053538	4.815569
259.681353	8000.030312	12.754343	-0.053545	4.815566
259.833755	8000.052024	12.759347	-0.053574	4.815572
259.745922	8000.013213	12.764352	-0.053558	4.815561
259.604299	8000.057893	12.769357	-0.053531	4.815574
259.607686	8000.041930	12.774362	-0.053532	4.815570
259.675308	8000.049443	12.779367	-0.053544	4.815572
259.694683	8000.054032	12.784371	-0.053548	4.815573
259.710780	8000.014781	12.789376	-0.053551	4.815561
259.781920	8000.042642	12.794381	-0.053564	4.815569
259.724654	8000.050253	12.799386	-0.053554	4.815572
259.595036	8000.025712	12.804391	-0.053530	4.815565
259.720954	8000.061942	12.809395	-0.053553	4.815575
259.587658	8000.033069	12.814400	-0.053528	4.815567
259.497305	8000.025188	12.819405	-0.053511	4.815565
259.688247	8000.038985	12.824410	-0.053547	4.815568
259.817013	8000.040020	12.829415	-0.053571	4.815568
259.748183	8000.043169	12.834419	-0.053558	4.815569
259.850928	8000.030964	12.839424	-0.053577	4.815565
259.947344	8000.037879	12.844429	-0.053595	4.815567
259.792510	8000.032149	12.849434	-0.053566	4.815566
259.674864	8000.015279	12.854439	-0.053545	4.815562
259.949120	8000.058202	12.859443	-0.053596	4.815573
259.910427	8000.021262	12.864448	-0.053588	4.815562
259.683489	8000.032511	12.869453	-0.053546	4.815567
259.932142	8000.054725	12.874458	-0.053593	4.815572
259.622275	8000.024038	12.879463	-0.053535	4.815564
259.868736	8000.044081	12.884467	-0.053581	4.815569
259.793660	8000.020430	12.889472	-0.053567	4.815562
259.796228	8000.058919	12.894477	-0.053567	4.815574
259.720142	8000.046999	12.899482	-0.053553	4.815571
259.614756	8000.022854	12.904487	-0.053533	4.815564
259.773671	8000.047875	12.909491	-0.053563	4.815571
259.856524	8000.007579	12.914496	-0.053579	4.815558
259.881939	8000.037897	12.919501	-0.053583	4.815567
259.931426	8000.054726	12.924506	-0.053593	4.815572
259.933724	8000.043017	12.929511	-0.053593	4.815568
259.775679	8000.034031	12.934515	-0.053564	4.815567
259.823171	8000.021992	12.939520	-0.053572	4.815563
259.836506	8000.045705	12.944525	-0.053575	4.815570
259.825695	8000.044462	12.949530	-0.053573	4.815569
259.827106	8000.016720	12.954535	-0.053573	4.815561
259.675787	8000.077261	12.959539	-0.053545	4.815580
259.787894	8000.017150	12.964544	-0.053566	4.815562
259.750119	8000.047506	12.969549	-0.053559	4.815571
259.835997	8000.033957	12.974554	-0.053575	4.815566
259.884331	8000.020864	12.979559	-0.053584	4.815562
259.957263	8000.067977	12.984563	-0.053598	4.815576
259.844950	8000.031971	12.989568	-0.053577	4.815566
259.988031	8000.052462	12.994573	-0.053603	4.815571
260.010437	8000.051761	12.999578	-0.053607	4.815571
259.854683	8000.039609	13.004583	-0.053578	4.815568
259.800774	8000.053682	13.009587	-0.053568	4.815572
259.842921	8000.041555	13.014592	-0.053576	4.815568
259.881779	8000.041123	13.019597	-0.053584	4.815568
259.914448	8000.050201	13.024602	-0.053590	4.815571
259.941240	8000.016465	13.029607	-0.053595	4.815561
260.012156	8000.063546	13.034611	-0.053608	4.815574
259.804890	8000.045213	13.039616	-0.053569	4.815570
259.900289	8000.043567	13.044621	-0.053587	4.815569
260.061512	8000.052607	13.049626	-0.053617	4.815571
259.879441	8000.036821	13.054631	-0.053583	4.815567
259.991848	8000.048269	13.059635	-0.053604	4.815570
260.049463	8000.048142	13.064640	-0.053615	4.815569
259.971839	8000.034061	13.069645	-0.053600	4.815566
259.921635	8000.059942	13.074650	-0.053591	4.815573
259.880653	8000.026168	13.079655	-0.053583	4.815564
259.849064	8000.077983	13.084659	-0.053578	4.815579
259.724599	8000.025759	13.089664	-0.053554	4.815564
259.697636	8000.036000	13.094669	-0.053549	4.815567
259.968089	8000.057502	13.099674	-0.053600	4.815572
259.771890	8000.021195	13.104679	-0.053563	4.815563
259.932066	8000.067596	13.109683	-0.053593	4.815576
259.970752	8000.056481	13.114688	-0.053600	4.815572
259.738016	8000.039869	13.119693	-0.053557	4.815568
259.628716	8000.056241	13.124698	-0.053537	4.815574
259.579421	8000.046895	13.129703	-0.053528	4.815571
259.613272	8000.069875	13.134707	-0.053534	4.815578
259.707731	8000.052195	13.139712	-0.053551	4.815572
259.762457	8000.054157	13.144717	-0.053562	4.815572
259.780833	8000.067274	13.149722	-0.053565	4.815576
259.874139	8000.034623	13.154727	-0.053582	4.815566
259.900198	8000.053205	13.159731	-0.053587	4.815572
260.027272	8000.073435	13.164736	-0.053611	4.815577
259.849931	8000.060931	13.169741	-0.053578	4.815574
259.874688	8000.077355	13.174746	-0.053583	4.815579
259.995523	8000.038746	13.179751	-0.053605	4.815567
260.128316	8000.071886	13.184755	-0.053630	4.815576
260.136830	8000.043191	13.189760	-0.053632	4.815567
259.950755	8000.056174	13.194765	-0.053597	4.815572
260.025944	8000.087306	13.199770	-0.053611	4.815581
259.827260	8000.042414	13.204775	-0.053574	4.815569
259.963862	8000.094839	13.209779	-0.053599	4.815583
260.064571	8000.043085	13.214784	-0.053618	4.815568
259.910396	8000.051250	13.219789	-0.053589	4.815571
259.951630	8000.038041	13.224794	-0.053597	4.815567
260.006902	8000.033604	13.229799	-0.053607	4.815565
259.944760	8000.042203	13.234803	-0.053596	4.815568
259.863337	8000.035535	13.239808	-0.053581	4.815567
259.877570	8000.049652	13.244813	-0.053583	4.815571
260.109170	8000.064113	13.249818	-0.053627	4.815574
259.898233	8000.031837	13.254823	-0.053587	4.815565
260.039349	8000.074724	13.259827	-0.053614	4.815577
259.906917	8000.053340	13.264832	-0.053589	4.815572
259.928668	8000.052628	13.269837	-0.053593	4.815571
259.870838	8000.049550	13.274842	-0.053582	4.815571
259.799512	7999.994989	13.279847	-0.053569	4.815555
259.871494	8000.051699	13.284851	-0.053582	4.815571
259.900771	8000.034022	13.289856	-0.053588	4.815566
259.925243	8000.026947	13.294861	-0.053592	4.815564
260.122229	8000.057931	13.299866	-0.053629	4.815572
260.063380	8000.008913	13.304871	-0.053618	4.815558
259.859787	8000.034426	13.309875	-0.053580	4.815566
260.095727	8000.043618	13.314880	-0.053624	4.815568
259.976008	8000.050209	13.319885	-0.053602	4.815570
259.890241	8000.064830	13.324890	-0.053586	4.815575
260.024474	8000.053138	13.329895	-0.053611	4.815571
260.066240	8000.067705	13.334899	-0.053619	4.815575
260.125887	8000.040913	13.339904	-0.053630	4.815567
259.835537	8000.055398	13.344909	-0.053576	4.815572
259.922084	8000.052540	13.349914	-0.053592	4.815571
259.893156	8000.032846	13.354919	-0.053587	4.815566
259.835759	8000.032978	13.359923	-0.053576	4.815566
259.841388	8000.020256	13.364928	-0.053577	4.815562
259.733215	7999.999269	13.369933	-0.053557	4.815557
259.799800	8000.033463	13.374938	-0.053569	4.815566
259.589141	8000.019347	13.379943	-0.053530	4.815563
259.706608	8000.007382	13.384947	-0.053552	4.815559
259.615009	8000.003752	13.389952	-0.053535	4.815558
259.632450	7999.992291	13.394957	-0.053538	4.815555
259.782700	8000.022511	13.399962	-0.053566	4.815563
259.948299	8000.024146	13.404967	-0.053597	4.815563
259.996569	8000.051634	13.409971	-0.053606	4.815571
260.003055	8000.041062	13.414976	-0.053607	4.815567
260.057403	8000.031271	13.419981	-0.053617	4.815564
260.105823	8000.053421	13.424986	-0.053626	4.815571
259.865179	8000.028136	13.429991	-0.053582	4.815564
260.053565	8000.061114	13.434995	-0.053617	4.815573
259.895629	8000.058538	13.440000	-0.053587	4.815573
259.960841	8000.036108	13.445005	-0.053599	4.815566
260.051872	8000.062158	13.450010	-0.053616	4.815573
260.226605	8000.013749	13.455015	-0.053649	4.815558
260.013622	8000.049789	13.460019	-0.053609	4.815570
260.041769	8000.040638	13.465024	-0.053615	4.815567
260.120023	8000.056868	13.470029	-0.053629	4.815572
260.055377	8000.062222	13.475034	-0.053617	4.815573
259.809637	8000.026173	13.480039	-0.053571	4.815564
260.001432	8000.058140	13.485043	-0.053607	4.815572
259.963563	8000.018008	13.490048	-0.053600	4.815561
259.939448	8000.052859	13.495053	-0.053596	4.815571
259.946832	8000.055116	13.500058	-0.053597	4.815572
260.085852	8000.030688	13.505063	-0.053623	4.815564
259.950748	8000.054115	13.510067	-0.053598	4.815572
259.744834	8000.039008	13.515072	-0.053559	4.815568
259.787921	8000.042916	13.520077	-0.053567	4.815569
259.924377	8000.054756	13.525082	-0.053593	4.815572
259.771766	8000.012752	13.530087	-0.053564	4.815560
259.998785	8000.070924	13.535091	-0.053607	4.815576
259.909985	8000.053457	13.540096	-0.053590	4.815572
259.884096	8000.048764	13.545101	-0.053585	4.815570
259.795189	8000.084692	13.550106	-0.053569	4.815581
259.951636	8000.043461	13.555111	-0.053598	4.815568
259.937203	8000.051770	13.560115	-0.053595	4.815571
259.980061	8000.075966	13.565120	-0.053603	4.815578
260.049199	8000.047192	13.570125	-0.053616	4.815569
260.064416	8000.094432	13.575130	-0.053619	4.815583
259.876964	8000.059335	13.580135	-0.053584	4.815573
259.856811	8000.062211	13.585139	-0.053580	4.815574
259.909655	8000.048124	13.590144	-0.053590	4.815570
259.874076	8000.049680	13.595149	-0.053584	4.815571
260.121779	8000.051588	13.600154	-0.053630	4.815570
259.901715	8000.029842	13.605159	-0.053589	4.815565
260.056894	8000.036648	13.610163	-0.053618	4.815566
259.883150	8000.029542	13.615168	-0.053585	4.815565
259.833526	8000.009510	13.620173	-0.053576	4.815559
260.024109	8000.066020	13.625178	-0.053612	4.815575
259.868332	8000.037847	13.630183	-0.053583	4.815567
259.914376	8000.065299	13.635187	-0.053591	4.815575
259.998659	8000.058132	13.640192	-0.053607	4.815572
260.013876	8000.045566	13.645197	-0.053610	4.815569
260.093283	8000.091718	13.650202	-0.053625	4.815582
260.136355	8000.062519	13.655207	-0.053633	4.815573
260.013721	8000.063723	13.660211	-0.053610	4.815574
260.090703	8000.039349	13.665216	-0.053624	4.815567
260.039567	8000.032108	13.670221	-0.053615	4.815565
260.005111	8000.057178	13.675226	-0.053608	4.815572
259.686663	8000.038098	13.680231	-0.053549	4.815568
260.011067	8000.079705	13.685235	-0.053609	4.815579
260.184221	8000.040882	13.690240	-0.053642	4.815567
259.748336	8000.033769	13.695245	-0.053561	4.815567
259.729295	8000.055886	13.700250	-0.053557	4.815573
259.857252	8000.033413	13.705255	-0.053581	4.815566
260.017260	8000.083016	13.710259	-0.053611	4.815580
260.166878	8000.047012	13.715264	-0.053639	4.815568
260.062694	8000.061333	13.720269	-0.053619	4.815573
260.085392	8000.037141	13.725274	-0.053623	4.815566
260.205441	8000.028422	13.730279	-0.053646	4.815563
260.172774	8000.043910	13.735283	-0.053640	4.815567
260.404520	8000.054102	13.740288	-0.053683	4.815569
260.120663	8000.047333	13.745293	-0.053630	4.815569
260.045868	8000.055725	13.750298	-0.053616	4.815572
259.918855	8000.050450	13.755303	-0.053592	4.815571
259.973281	8000.063087	13.760307	-0.053603	4.815574
260.010141	8000.064758	13.765312	-0.053610	4.815574
259.845925	8000.030040	13.770317	-0.053579	4.815565
260.163599	8000.055517	13.775322	-0.053638	4.815571
260.047540	8000.041876	13.780327	-0.053617	4.815567
259.958842	8000.047906	13.785331	-0.053600	4.815570
260.025978	8000.052207	13.790336	-0.053613	4.815571
260.026772	8000.043677	13.795341	-0.053613	4.815568
259.884142	8000.031739	13.800346	-0.053586	4.815565
260.001407	8000.017634	13.805351	-0.053608	4.815561
260.092086	8000.069310	13.810355	-0.053625	4.815575
260.082110	8000.054197	13.815360	-0.053623	4.815571
259.943970	8000.016701	13.820365	-0.053597	4.815561
260.073395	8000.046581	13.825370	-0.053621	4.815569
259.906884	8000.023574	13.830375	-0.053590	4.815563
259.810234	8000.018794	13.835379	-0.053572	4.815562
259.849889	8000.007694	13.840384	-0.053580	4.815558
259.955653	8000.023305	13.845389	-0.053600	4.815562
259.782841	8000.064272	13.850394	-0.053567	4.815575
259.830744	8000.039424	13.855399	-0.053576	4.815568
259.943560	8000.069034	13.860403	-0.053597	4.815576
260.042483	8000.040747	13.865408	-0.053616	4.815567
259.889154	8000.001935	13.870413	-0.053587	4.815557
259.806133	8000.025144	13.875418	-0.053572	4.815564
259.817117	8000.009305	13.880423	-0.053574	4.815559
259.904305	8000.055583	13.885427	-0.053590	4.815572
260.113648	8000.051526	13.890432	-0.053629	4.815570
260.045709	8000.017311	13.895437	-0.053616	4.815560
260.125782	8000.060270	13.900442	-0.053631	4.815572
259.869982	8000.024057	13.905447	-0.053584	4.815563
260.158885	8000.073628	13.910451	-0.053638	4.815576
260.160697	8000.066183	13.915456	-0.053638	4.815574
259.952732	8000.045703	13.920461	-0.053599	4.815569
260.192805	8000.072050	13.925466	-0.053644	4.815576
260.078650	8000.045624	13.930471	-0.053623	4.815568
260.062218	8000.056037	13.935475	-0.053620	4.815572
259.981132	8000.042967	13.940480	-0.053605	4.815568
259.907939	8000.050318	13.945485	-0.053591	4.815571
259.908564	8000.052465	13.950490	-0.053591	4.815571
259.921326	8000.037723	13.955495	-0.053593	4.815567
259.890224	8000.032945	13.960499	-0.053588	4.815566
259.875038	8000.046582	13.965504	-0.053585	4.815570
260.021131	8000.029744	13.970509	-0.053612	4.815564
260.129343	8000.034715	13.975514	-0.053632	4.815565
259.955932	8000.014799	13.980519	-0.053600	4.815560
259.956486	8000.059663	13.985523	-0.053600	4.815573
260.064235	8000.069967	13.990528	-0.053620	4.815576
260.023739	8000.039404	13.995533	-0.053613	4.815567
259.950212	8000.052089	14.000538	-0.053599	4.815571
259.899499	8000.021359	14.005543	-0.053590	4.815562
260.026588	8000.052270	14.010547	-0.053613	4.815571
259.974884	8000.050359	14.015552	-0.053604	4.815570
259.968066	8000.045977	14.020557	-0.053602	4.815569
260.016377	8000.069194	14.025562	-0.053611	4.815576
259.962633	8000.043755	14.030567	-0.053601	4.815568
259.816624	8000.046713	14.035571	-0.053574	4.815570
259.871780	8000.038003	14.040576	-0.053584	4.815567
259.980957	7999.999204	14.045581	-0.053605	4.815555
260.000591	8000.049719	14.050586	-0.053609	4.815570
259.882088	8000.038175	14.055591	-0.053586	4.815567
259.989253	8000.065556	14.060595	-0.053606	4.815575
259.970410	8000.046026	14.065600	-0.053603	4.815569
259.872992	8000.020943	14.070605	-0.053585	4.815562
259.921876	8000.030285	14.075610	-0.053594	4.815565
260.063025	8000.026182	14.080615	-0.053620	4.815563
259.993735	8000.048548	14.085619	-0.053607	4.815570
259.952719	8000.031860	14.090624	-0.053600	4.815565
259.970751	8000.031088	14.095629	-0.053603	4.815565
259.998595	8000.078534	14.100634	-0.053608	4.815578
259.713226	8000.017276	14.105639	-0.053555	4.815562
259.799287	8000.041109	14.110643	-0.053571	4.815568
260.021489	8000.030853	14.115648	-0.053613	4.815564
259.826162	8000.044753	14.120653	-0.053576	4.815569
259.969482	8000.079133	14.125658	-0.053603	4.815579
260.117289	8000.036692	14.130663	-0.053630	4.815566
259.925581	8000.079486	14.135667	-0.053595	4.815579
259.989255	8000.054896	14.140672	-0.053607	4.815572
259.869596	8000.059352	14.145677	-0.053584	4.815573
259.773200	8000.064188	14.150682	-0.053566	4.815575
259.736367	8000.042229	14.155687	-0.053560	4.815569
260.001031	8000.063637	14.160691	-0.053609	4.815574
260.217387	8000.054354	14.165696	-0.053649	4.815570
260.050058	8000.025993	14.170701	-0.053618	4.815563
259.921102	8000.044180	14.175706	-0.053594	4.815569
259.958729	8000.021301	14.180711	-0.053601	4.815562
259.809767	8000.037026	14.185715	-0.053573	4.815567
259.906494	8000.045014	14.190720	-0.053591	4.815569
259.928949	8000.030430	14.195725	-0.053596	4.815565
259.993690	8000.060323	14.200730	-0.053608	4.815573
259.935963	8000.034819	14.205735	-0.053597	4.815566
259.828288	8000.043742	14.210739	-0.053577	4.815569
259.986042	8000.055930	14.215744	-0.053606	4.815572
259.932867	8000.040111	14.220749	-0.053596	4.815567
259.933526	8000.084978	14.225754	-0.053597	4.815581
260.084050	8000.029766	14.230759	-0.053625	4.815564
259.928362	8000.035770	14.235763	-0.053596	4.815566
259.883671	8000.043585	14.240768	-0.053587	4.815569
260.011329	8000.009359	14.245773	-0.053611	4.815558
259.869227	8000.056167	14.250778	-0.053585	4.815572
259.761420	8000.012759	14.255783	-0.053565	4.815560
259.796704	8000.037899	14.260787	-0.053571	4.815567
259.992298	8000.062452	14.265792	-0.053608	4.815574
260.039818	7999.039084	14.270797	-0.053616	4.815274
260.122298	7995.969441	14.275802	-0.053629	4.814376
259.929181	7990.553995	14.280807	-0.053590	4.812794
259.920222	7983.877922	14.285811	-0.053584	4.810840
259.969863	7976.672266	14.290816	-0.053588	4.808731
259.696948	7968.995718	14.295821	-0.053532	4.806485
259.596533	7961.196604	14.300826	-0.053509	4.804200
259.505923	7953.372641	14.305831	-0.053487	4.801907
259.490367	7945.333254	14.310835	-0.053479	4.799550
259.724210	7937.498340	14.315840	-0.053517	4.797250
259.689239	7929.384574	14.320845	-0.053505	4.794869
259.462933	7921.445344	14.325850	-0.053458	4.792538
259.659531	7913.390734	14.330855	-0.053489	4.790171
259.602624	7905.413992	14.335859	-0.053474	4.787826
259.408818	7897.366068	14.340864	-0.053432	4.785460
259.310345	7889.400940	14.345869	-0.053409	4.783117
259.386438	7881.374256	14.350874	-0.053418	4.780753
259.283669	7873.439223	14.355879	-0.053393	4.778417
259.456086	7865.384615	14.360883	-0.053420	4.776042
259.334860	7857.408515	14.365888	-0.053392	4.773691
259.296818	7849.333759	14.370893	-0.053380	4.771309
259.168943	7841.356062	14.375898	-0.053351	4.768955
259.470412	7833.414063	14.380903	-0.053402	4.766609
259.080030	7825.323813	14.385907	-0.053324	4.764221
259.050391	7817.453270	14.390912	-0.053314	4.761894
259.206596	7809.337565	14.395917	-0.053337	4.759494
259.358455	7801.430512	14.400922	-0.053360	4.757154
259.041548	7793.365939	14.405927	-0.053296	4.754768
258.911275	7785.302352	14.410931	-0.053267	4.752380
258.993481	7777.303133	14.415936	-0.053277	4.750009
258.834599	7769.336881	14.420941	-0.053242	4.747648
258.762214	7761.351370	14.425946	-0.053223	4.745280
258.699535	7753.346843	14.430951	-0.053207	4.742905
258.884738	7745.306826	14.435955	-0.053236	4.740517
258.877534	7737.381308	14.440960	-0.053229	4.738163
258.741585	7729.352413	14.445965	-0.053199	4.735777
258.870450	7721.353253	14.450970	-0.053218	4.733398
258.836001	7713.292545	14.455975	-0.053206	4.731000
258.627846	7705.264759	14.460979	-0.053162	4.728611
258.816183	7697.347394	14.465984	-0.053192	4.726253
258.725445	7689.253380	14.470989	-0.053170	4.723841
258.723382	7681.318216	14.475994	-0.053164	4.721476
258.630130	7673.328713	14.480999	-0.053142	4.719093
258.575341	7665.345699	14.486003	-0.053126	4.716711
258.475298	7657.372655	14.491008	-0.053102	4.714331
258.481480	7649.319882	14.496013	-0.053098	4.711925
258.424745	7641.279102	14.501018	-0.053083	4.709522
258.498003	7633.336323	14.506023	-0.053091	4.707147
258.331291	7625.264341	14.511027	-0.053055	4.704732
258.283662	7617.308988	14.516032	-0.053041	4.702351
258.434735	7609.267341	14.521037	-0.053064	4.699943
258.416719	7601.331765	14.526042	-0.053055	4.697565
258.227225	7593.316861	14.531047	-0.053015	4.695162
258.233106	7585.267825	14.536051	-0.053010	4.692748
258.189689	7577.284002	14.541056	-0.052997	4.690352
257.988759	7569.287761	14.546061	-0.052955	4.687952
258.008002	7561.283450	14.551066	-0.052953	4.685547
258.129983	7553.327431	14.556071	-0.052970	4.683156
258.028976	7545.255928	14.561075	-0.052946	4.680729
258.138955	7537.338087	14.566080	-0.052962	4.678346
258.025785	7529.275910	14.571085	-0.052935	4.675920
257.973013	7521.225512	14.576090	-0.052920	4.673495
257.908775	7513.157516	14.581095	-0.052903	4.671064
257.914428	7505.181019	14.586099	-0.052899	4.668659
257.785026	7497.250499	14.591104	-0.052870	4.666267
257.561959	7489.231693	14.596109	-0.052823	4.663847
257.664840	7481.253513	14.601114	-0.052837	4.661438
257.560845	7473.227033	14.606119	-0.052812	4.659013
257.225486	7465.247368	14.611123	-0.052745	4.656601
257.328665	7457.258920	14.616128	-0.052759	4.654185
257.229497	7449.200751	14.621133	-0.052735	4.651747
257.267364	7441.242082	14.626138	-0.052737	4.649337
257.110726	7433.196353	14.631143	-0.052703	4.646900
257.150130	7425.120370	14.636147	-0.052705	4.644453
257.525412	7417.257301	14.641152	-0.052769	4.642068
257.470157	7409.220316	14.646157	-0.052754	4.639630
257.342691	7401.290278	14.651162	-0.052725	4.637223
257.462228	7393.224024	14.656167	-0.052742	4.634773
257.285213	7385.206765	14.661171	-0.052704	4.632337
257.337779	7377.195112	14.666176	-0.052708	4.629901
257.417067	7369.176406	14.671181	-0.052718	4.627462
257.303036	7361.173020	14.676186	-0.052692	4.625026
257.334420	7353.225249	14.681191	-0.052692	4.622606
257.175300	7345.169882	14.686195	-0.052657	4.620152
257.112309	7337.239712	14.691200	-0.052641	4.617734
256.921938	7329.168400	14.696205	-0.052600	4.615273
257.014231	7321.191452	14.701210	-0.052612	4.612838
256.951091	7313.131843	14.706215	-0.052595	4.610378
256.820709	7305.166514	14.711219	-0.052565	4.607944
256.870176	7297.179797	14.716224	-0.052569	4.605503
256.938198	7289.168711	14.721229	-0.052577	4.603053
257.037400	7281.141435	14.726234	-0.052590	4.600597
256.812513	7273.208549	14.731239	-0.052543	4.598169
256.563489	7265.150572	14.736243	-0.052491	4.595700
257.069005	7257.144661	14.741248	-0.052580	4.593247
256.833134	7249.101463	14.746253	-0.052531	4.590781
256.714687	7241.102123	14.751258	-0.052504	4.588327
256.848760	7233.104519	14.756263	-0.052524	4.585872
256.702906	7225.113867	14.761267	-0.052491	4.583418
256.713783	7217.149493	14.766272	-0.052488	4.580970
256.749815	7209.153778	14.771277	-0.052490	4.578512
256.560531	7201.176221	14.776282	-0.052449	4.576058
256.534147	7193.153828	14.781287	-0.052439	4.573589
256.482184	7185.089250	14.786291	-0.052424	4.571105
256.438985	7177.118194	14.791296	-0.052411	4.568649
256.371793	7169.123193	14.796301	-0.052393	4.566184
256.267261	7161.152929	14.801306	-0.052369	4.563725
256.240570	7153.158367	14.806311	-0.052359	4.561258
256.244985	7145.169024	14.811315	-0.052354	4.558791
256.264027	7137.207181	14.816320	-0.052353	4.556331
256.062647	7129.122458	14.821325	-0.052310	4.553832
256.185487	7121.070928	14.826330	-0.052327	4.551342
256.141080	7113.115398	14.831335	-0.052314	4.548880
256.087615	7105.053367	14.836339	-0.052299	4.546383
256.118887	7097.130324	14.841344	-0.052299	4.543929
255.841914	7089.108604	14.846349	-0.052243	4.541442
255.864601	7081.115786	14.851354	-0.052242	4.538963
256.023514	7073.139576	14.856359	-0.052266	4.536488
255.971437	7065.122754	14.861363	-0.052251	4.533999
255.882527	7057.097541	14.866368	-0.052229	4.531506
255.668994	7049.116785	14.871373	-0.052185	4.529025
255.719483	7041.107563	14.876378	-0.052189	4.526534
255.751325	7033.118919	14.881383	-0.052189	4.524048
255.629659	7025.118736	14.886387	-0.052162	4.521557
255.812043	7017.120746	14.891392	-0.052190	4.519066
255.580669	7009.162318	14.896397	-0.052142	4.516585
255.431125	7001.065603	14.901402	-0.052109	4.514060
255.441470	6993.006207	14.906407	-0.052106	4.511545
255.334492	6985.001262	14.911411	-0.052081	4.509045
255.424328	6977.045104	14.916416	-0.052092	4.506560
255.232570	6969.040818	14.921421	-0.052051	4.504058
255.236267	6961.084249	14.926426	-0.052047	4.501570
255.122462	6953.046365	14.931431	-0.052020	4.499054
255.149522	6945.091485	14.936435	-0.052020	4.496564
255.304992	6937.081016	14.941440	-0.052044	4.494055
255.179607	6929.012937	14.946445	-0.052015	4.491526
255.095216	6921.021711	14.951450	-0.051994	4.489020
255.053213	6913.068385	14.956455	-0.051981	4.486524
254.837024	6905.022865	14.961459	-0.051936	4.483997
254.958148	6897.079816	14.966464	-0.051953	4.481503
254.983405	6889.063716	14.971469	-0.051953	4.478983
254.974035	6881.068376	14.976474	-0.051946	4.476469
254.735229	6873.055258	14.981479	-0.051896	4.473946
254.794118	6865.018658	14.986483	-0.051902	4.471416
254.845029	6857.008479	14.991488	-0.051906	4.468893
254.945723	6849.004218	14.996493	-0.051920	4.466371
254.866487	6840.984787	15.001498	-0.051900	4.463841
254.807203	6833.065644	15.006503	-0.051884	4.461342
254.676357	6825.031236	15.011507	-0.051854	4.458805
254.815648	6817.039630	15.016512	-0.051875	4.456281
254.667649	6809.063010	15.021517	-0.051842	4.453759
254.679678	6801.009008	15.026522	-0.051839	4.451211
254.709903	6793.033356	15.031527	-0.051839	4.448687
254.581445	6784.982489	15.036531	-0.051810	4.446138
254.588293	6777.038927	15.041536	-0.051806	4.443621
254.505829	6768.998678	15.046541	-0.051786	4.441072
254.454648	6761.032523	15.051546	-0.051771	4.438545
254.466129	6753.022859	15.056551	-0.051768	4.436003
254.462397	6744.965911	15.061555	-0.051762	4.433445
254.354750	6736.957344	15.066560	-0.051737	4.430900
254.182524	6728.956325	15.071565	-0.051700	4.428355
254.251396	6720.949583	15.076570	-0.051707	4.425809
254.342351	6713.025552	15.081575	-0.051719	4.423287
254.104844	6704.985501	15.086579	-0.051670	4.420725
254.123621	6697.002141	15.091584	-0.051668	4.418181
254.115017	6688.974857	15.096589	-0.051661	4.415622
253.966980	6680.941697	15.101594	-0.051628	4.413059
253.880762	6672.948471	15.106599	-0.051607	4.410507
253.980325	6664.967692	15.111603	-0.051620	4.407958
253.809783	6656.987079	15.116608	-0.051583	4.405407
253.648116	6649.008092	15.121613	-0.051548	4.402855
253.805952	6640.972905	15.126618	-0.051572	4.400285
253.734730	6633.029066	15.131623	-0.051554	4.397741
253.602211	6624.971054	15.136627	-0.051524	4.395159
253.757425	6617.003463	15.141632	-0.051548	4.392606
253.676359	6608.908300	15.146637	-0.051527	4.390010
253.812116	6600.961032	15.151642	-0.051547	4.387460
253.721375	6592.965001	15.156647	-0.051525	4.384892
253.699724	6585.020063	15.161651	-0.051516	4.382340
253.640511	6576.991125	15.166656	-0.051500	4.379759
253.624341	6569.014682	15.171661	-0.051492	4.377193
253.636089	6560.973559	15.176666	-0.051489	4.374605
253.573922	6552.980256	15.181671	-0.051472	4.372031
253.266899	6544.928516	15.186675	-0.051410	4.369435
253.398598	6536.973027	15.191680	-0.051429	4.366870
253.299375	6528.975342	15.196685	-0.051405	4.364290
253.189055	6521.049367	15.201690	-0.051380	4.361731
253.132582	6512.963727	15.206695	-0.051364	4.359119
253.185964	6505.003431	15.211699	-0.051369	4.356547
253.118421	6496.951801	15.216704	-0.051351	4.353942
253.068582	6488.864151	15.221709	-0.051336	4.351325
253.123408	6480.888189	15.226714	-0.051341	4.348743
253.129557	6472.949748	15.231719	-0.051337	4.346172
253.102306	6464.928122	15.236723	-0.051327	4.343572
253.337759	6456.962572	15.241728	-0.051366	4.340990
253.223621	6448.952349	15.246733	-0.051339	4.338389
252.969658	6440.988423	15.251738	-0.051287	4.335801
252.895391	6432.956318	15.256743	-0.051268	4.333191
252.831388	6424.896227	15.261747	-0.051250	4.330570
252.863280	6416.953109	15.266752	-0.051251	4.327986
252.655869	6408.929910	15.271757	-0.051207	4.325373
252.833665	6400.940400	15.276762	-0.051235	4.322772
252.797937	6392.960455	15.281767	-0.051223	4.320171
252.548343	6384.960538	15.286771	-0.051172	4.317561
252.553188	6376.960682	15.291776	-0.051167	4.314951
252.667959	6368.923934	15.296781	-0.051184	4.312327
252.592082	6360.887892	15.301786	-0.051164	4.309702
252.733078	6352.948110	15.306791	-0.051185	4.307107
252.590219	6344.917704	15.311795	-0.051154	4.304479
252.663866	6336.946209	15.316800	-0.051162	4.301871
252.519305	6328.915221	15.321805	-0.051130	4.299240
252.455566	6320.936777	15.326810	-0.051113	4.296625
252.457161	6312.907366	15.331815	-0.051108	4.293992
252.262215	6304.878231	15.336819	-0.051066	4.291356
252.230953	6296.954613	15.341824	-0.051055	4.288754
252.290463	6288.905284	15.346829	-0.051061	4.286111
252.175385	6280.908996	15.351834	-0.051035	4.283481
251.981515	6272.909242	15.356839	-0.050993	4.280849
252.010346	6264.927744	15.361843	-0.050994	4.278222
252.200213	6256.917599	15.366848	-0.051024	4.275586
252.150854	6248.902458	15.371853	-0.051009	4.272944
251.909436	6240.827297	15.376858	-0.050959	4.270280
252.025202	6232.887840	15.381863	-0.050976	4.267661
252.064538	6224.831405	15.386867	-0.050978	4.265002
251.821058	6216.911347	15.391872	-0.050927	4.262384
251.772778	6208.902228	15.396877	-0.050913	4.259736
251.776591	6200.905191	15.401882	-0.050908	4.257091
251.700877	6192.912481	15.406887	-0.050889	4.254445
251.602516	6184.863206	15.411891	-0.050866	4.251778
251.763976	6176.900338	15.416896	-0.050890	4.249141
251.577612	6168.881499	15.421901	-0.050851	4.246481
251.285959	6160.907423	15.426906	-0.050791	4.243832
251.532075	6152.919426	15.431911	-0.050832	4.241183
251.409126	6144.941239	15.436915	-0.050804	4.238531
251.617721	6136.932274	15.441920	-0.050837	4.235871
251.566857	6128.905752	15.446925	-0.050823	4.233201
251.405259	6120.847230	15.451930	-0.050787	4.230517
251.483401	6112.938673	15.456935	-0.050797	4.227884
251.470835	6104.868184	15.461939	-0.050789	4.225194
251.463930	6096.961790	15.466944	-0.050783	4.222558
251.191496	6088.908345	15.471949	-0.050727	4.219868
251.188443	6080.941775	15.476954	-0.050721	4.217208
251.422053	6072.948777	15.481959	-0.050759	4.214540
251.163389	6064.913224	15.486963	-0.050706	4.211851
251.229247	6056.914002	15.491968	-0.050713	4.209176
251.312312	6048.923977	15.496973	-0.050723	4.206502
251.303811	6040.889672	15.501978	-0.050716	4.203811
251.183765	6032.958063	15.506983	-0.050689	4.201151
251.116301	6024.928443	15.511987	-0.050671	4.198457
250.983292	6016.958168	15.516992	-0.050641	4.195781
250.863593	6008.829971	15.521997	-0.050614	4.193050
250.826645	6000.816856	15.527002	-0.050602	4.190357
250.994101	5992.884931	15.532007	-0.050628	4.187692
250.896759	5984.866407	15.537011	-0.050604	4.184993
250.931278	5976.928520	15.542016	-0.050605	4.182321
250.746543	5968.871350	15.547021	-0.050566	4.179605
250.897711	5960.929687	15.552026	-0.050589	4.176929
250.649775	5952.920272	15.557031	-0.050537	4.174224
250.509916	5944.863543	15.562035	-0.050506	4.171503
250.579161	5936.877179	15.567040	-0.050514	4.168806
250.554531	5928.900059	15.572045	-0.050504	4.166110
250.489425	5920.863056	15.577050	-0.050487	4.163391
250.670544	5912.927127	15.582055	-0.050515	4.160707
250.464228	5904.905432	15.587059	-0.050472	4.157988
250.433766	5896.917994	15.592064	-0.050461	4.155281
250.150555	5888.867257	15.597069	-0.050403	4.152548
250.302153	5880.832495	15.602074	-0.050426	4.149823
250.163179	5872.882109	15.607079	-0.050395	4.147122
249.924571	5864.879865	15.612083	-0.050345	4.144401
250.177895	5856.913230	15.617088	-0.050387	4.141695
250.274337	5848.881171	15.622093	-0.050400	4.138964
250.241815	5840.891102	15.627098	-0.050389	4.136243
250.182017	5832.894470	15.632103	-0.050372	4.133518
250.097958	5824.830781	15.637107	-0.050351	4.130768
250.211749	5816.886966	15.642112	-0.050367	4.128060
249.964081	5808.875645	15.647117	-0.050316	4.125322
250.016637	5800.897050	15.652122	-0.050321	4.122598
249.957835	5792.907757	15.657127	-0.050305	4.119866
249.840385	5784.923243	15.662131	-0.050278	4.117134
249.753271	5776.879117	15.667136	-0.050256	4.114380
249.878742	5768.824209	15.672141	-0.050274	4.111623
249.586528	5760.867884	15.677146	-0.050215	4.108892
249.796114	5752.845093	15.682151	-0.050248	4.106144
249.856224	5744.841498	15.687155	-0.050254	4.103398
249.776348	5736.907700	15.692160	-0.050234	4.100672
249.627431	5728.923757	15.697165	-0.050201	4.097927
249.594903	5720.905317	15.702170	-0.050190	4.095169
249.636759	5712.907536	15.707175	-0.050193	4.092418
249.398212	5704.872644	15.712179	-0.050143	4.089648
249.436322	5696.912105	15.717184	-0.050145	4.086905
249.318933	5688.895173	15.722189	-0.050118	4.084140
249.256093	5680.936734	15.727194	-0.050101	4.081393
249.260718	5672.954774	15.732199	-0.050097	4.078637
249.355956	5664.922178	15.737203	-0.050109	4.075863
249.427673	5656.895969	15.742208	-0.050117	4.073089
249.201525	5648.866544	15.747213	-0.050070	4.070308
249.214446	5640.909586	15.752218	-0.050067	4.067554
249.244376	5632.913180	15.757223	-0.050068	4.064784
249.016184	5624.981457	15.762227	-0.050020	4.062031
248.939394	5616.906811	15.767232	-0.050001	4.059229
249.233441	5608.922164	15.772237	-0.050050	4.056461
249.197609	5600.897326	15.777242	-0.050038	4.053673
249.077006	5592.907621	15.782247	-0.050011	4.050893
249.132234	5584.914255	15.787251	-0.050016	4.048114
249.162316	5576.896947	15.792256	-0.050016	4.045323
249.015604	5568.949123	15.797261	-0.049984	4.042552
249.072997	5560.905885	15.802266	-0.049989	4.039749
249.065764	5552.981031	15.807271	-0.049983	4.036985
248.730662	5544.897824	15.812275	-0.049915	4.034158
248.765246	5536.829445	15.817280	-0.049916	4.031340
249.004565	5528.859579	15.822285	-0.049955	4.028558
248.865215	5520.829581	15.827290	-0.049924	4.025747
248.669493	5512.917393	15.832295	-0.049883	4.022974
248.625385	5504.898937	15.837299	-0.049869	4.020165
248.833804	5496.917672	15.842304	-0.049903	4.017370
248.630136	5488.910373	15.847309	-0.049860	4.014558
248.510952	5480.874777	15.852314	-0.049832	4.011736
248.565938	5472.853077	15.857319	-0.049837	4.008919
248.328908	5464.886549	15.862323	-0.049788	4.006115
248.480015	5456.894845	15.867328	-0.049811	4.003306
248.445170	5448.932211	15.872333	-0.049799	4.000502
248.326900	5440.934687	15.877338	-0.049772	3.997683
248.144738	5432.943132	15.882343	-0.049733	3.994863
248.137242	5424.868764	15.887347	-0.049726	3.992014
248.348154	5416.856385	15.892352	-0.049760	3.989189
248.209837	5408.875516	15.897357	-0.049730	3.986368
248.216276	5400.846833	15.902362	-0.049725	3.983529
248.219377	5392.918425	15.907367	-0.049721	3.980725
248.120631	5384.919291	15.912371	-0.049697	3.977891
247.925993	5376.921617	15.917376	-0.049656	3.975054
247.867681	5368.919766	15.922381	-0.049640	3.972216
247.847795	5360.897208	15.927386	-0.049631	3.969370
247.959541	5352.946216	15.932391	-0.049647	3.966549
247.678206	5344.943260	15.937395	-0.049589	3.963701
247.800634	5336.941674	15.942400	-0.049607	3.960858
247.748065	5328.998100	15.947405	-0.049592	3.958030
247.700880	5320.938137	15.952410	-0.049578	3.955160
247.822923	5312.919603	15.957415	-0.049595	3.952305
247.510457	5304.888681	15.962419	-0.049532	3.949436
247.318267	5296.947911	15.967424	-0.049491	3.946599
247.435558	5288.946996	15.972429	-0.049507	3.943743
247.349471	5280.968883	15.977434	-0.049486	3.940891
247.424102	5273.015659	15.982439	-0.049495	3.938048
247.275631	5264.964169	15.987443	-0.049462	3.935164
247.444863	5256.943704	15.992448	-0.049488	3.932294
247.298407	5248.937926	15.997453	-0.049456	3.929423
247.060351	5240.957482	16.002458	-0.049406	3.926556
247.386578	5232.963096	16.007463	-0.049462	3.923692
247.465468	5224.975691	16.012467	-0.049471	3.920825
247.326401	5217.006961	16.017472	-0.049440	3.917958
247.318139	5208.994050	16.022477	-0.049434	3.915075
247.318129	5200.944148	16.027482	-0.049428	3.912178
247.236687	5192.971123	16.032487	-0.049408	3.909304
246.911813	5185.012284	16.037491	-0.049342	3.906428
247.056635	5176.967558	16.042496	-0.049364	3.903529
247.103601	5168.969301	16.047501	-0.049368	3.900642
246.987122	5160.991560	16.052506	-0.049341	3.897757
247.205551	5152.979734	16.057511	-0.049376	3.894864
246.898433	5144.948033	16.062515	-0.049314	3.891952
246.793505	5136.918668	16.067520	-0.049289	3.889042
246.946947	5128.985830	16.072525	-0.049312	3.886170
246.802168	5120.980050	16.077530	-0.049280	3.883264
246.717183	5112.978851	16.082535	-0.049259	3.880358
246.659524	5105.014869	16.087539	-0.049243	3.877465
246.751495	5097.002433	16.092544	-0.049255	3.874554
246.784221	5088.723800	16.097549	-0.049256	3.871543
246.486186	5080.806465	16.102554	-0.049195	3.868655
246.616324	5072.877833	16.107559	-0.049214	3.865769
246.468810	5064.919759	16.112563	-0.049182	3.862865
246.533882	5056.935541	16.117568	-0.049189	3.859953
246.358698	5048.993639	16.122573	-0.049151	3.857049
246.525429	5040.962034	16.127578	-0.049177	3.854118
246.495963	5032.966988	16.132583	-0.049166	3.851193
246.202989	5024.988438	16.137587	-0.049106	3.848267
246.444658	5016.975998	16.142592	-0.049146	3.845338
246.431006	5009.006016	16.147597	-0.049138	3.842416
246.259596	5000.996532	16.152602	-0.049101	3.839475
246.269088	4993.053617	16.157607	-0.049098	3.836559
246.080974	4985.025996	16.162611	-0.049058	3.833606
246.068977	4976.980211	16.167616	-0.049050	3.830647
246.072968	4969.022013	16.172621	-0.049046	3.827719
245.878707	4961.006672	16.177626	-0.049004	3.824764
245.886765	4953.046975	16.182631	-0.049001	3.821831
245.832863	4945.057189	16.187635	-0.048985	3.818883
245.937258	4937.050925	16.192640	-0.049000	3.815930
245.986589	4929.043029	16.197645	-0.049004	3.812973
245.585180	4921.019433	16.202650	-0.048924	3.809998
245.659088	4913.070704	16.207655	-0.048932	3.807059
245.823946	4905.050271	16.212659	-0.048958	3.804093
245.707466	4897.080354	16.217664	-0.048931	3.801138
245.579009	4889.111507	16.222669	-0.048902	3.798180
245.650355	4881.056382	16.227674	-0.048910	3.795192
245.651172	4873.047053	16.232679	-0.048905	3.792218
245.411816	4865.033964	16.237683	-0.048855	3.789234
245.571732	4857.047914	16.242688	-0.048880	3.786267
245.597065	4849.055168	16.247693	-0.048879	3.783292
245.547323	4841.067354	16.252698	-0.048865	3.780315
245.457617	4833.127608	16.257703	-0.048843	3.777352
245.467169	4825.055158	16.262707	-0.048839	3.774340
245.296246	4817.063617	16.267712	-0.048802	3.771352
245.001114	4809.087724	16.272717	-0.048742	3.768364
245.206278	4801.048519	16.277722	-0.048775	3.765362
245.251849	4793.104619	16.282727	-0.048779	3.762389
245.094946	4785.089467	16.287731	-0.048744	3.759382
245.085904	4777.127450	16.292736	-0.048737	3.756397
245.087481	4769.065497	16.297741	-0.048732	3.753372
245.163543	4761.032850	16.302746	-0.048741	3.750357
244.991383	4753.072735	16.307751	-0.048704	3.747361
244.882815	4745.057851	16.312755	-0.048679	3.744343
244.959771	4737.129048	16.317760	-0.048688	3.741360
244.790059	4729.128440	16.322765	-0.048651	3.738342
244.718187	4721.093448	16.327770	-0.048632	3.735310
244.645253	4713.122143	16.332775	-0.048614	3.732301
244.400704	4705.080603	16.337779	-0.048563	3.729258
244.750236	4697.104553	16.342784	-0.048623	3.726251
244.559071	4689.162686	16.347789	-0.048582	3.723242
244.484422	4681.134974	16.352794	-0.048563	3.720201
244.555056	4673.193489	16.357799	-0.048571	3.717193
244.385024	4665.157043	16.362803	-0.048534	3.714142
244.378872	4657.020501	16.367808	-0.048528	3.711053
244.311820	4649.075427	16.372813	-0.048510	3.708034
244.245666	4641.090832	16.377818	-0.048492	3.704997
244.365388	4633.166328	16.382823	-0.048509	3.701985
244.235082	4625.157202	16.387827	-0.048480	3.698932
244.307794	4617.175841	16.392832	-0.048488	3.695892
244.276786	4609.194747	16.397837	-0.048477	3.692847
244.178020	4601.141335	16.402842	-0.048454	3.689770
244.313760	4593.176390	16.407847	-0.048474	3.686731
244.188780	4585.172402	16.412851	-0.048445	3.683667
243.981846	4577.207495	16.417856	-0.048402	3.680614
244.120288	4569.249075	16.422861	-0.048422	3.677569
243.876265	4561.207167	16.427866	-0.048372	3.674480
243.895980	4553.225213	16.432871	-0.048370	3.671418
243.824855	4545.178814	16.437875	-0.048352	3.668327
243.798305	4537.196321	16.442880	-0.048342	3.665259
243.905710	4529.235809	16.447885	-0.048356	3.662200
243.980705	4521.193307	16.452890	-0.048365	3.659106
244.006422	4513.225734	16.457895	-0.048365	3.656037
243.960466	4505.218748	16.462899	-0.048351	3.652948
243.825853	4497.175300	16.467904	-0.048321	3.649841
243.711427	4489.247265	16.472909	-0.048294	3.646775
243.671029	4481.216720	16.477914	-0.048281	3.643670
243.882736	4473.269211	16.482919	-0.048316	3.640601
243.786644	4465.282726	16.487923	-0.048293	3.637506
243.725280	4457.239482	16.492928	-0.048276	3.634387
243.605380	4449.236212	16.497933	-0.048248	3.631279
243.513108	4441.191302	16.502938	-0.048226	3.628153
243.463159	4433.254818	16.507943	-0.048212	3.625068
243.418618	4425.262950	16.512947	-0.048198	3.621959
243.364507	4417.265816	16.517952	-0.048183	3.618845
243.524587	4409.300537	16.522957	-0.048207	3.615746
243.290836	4401.280241	16.527962	-0.048159	3.612613
243.314437	4393.280744	16.532967	-0.048158	3.609492
243.437199	4385.258736	16.537971	-0.048176	3.606362
243.221048	4377.292564	16.542976	-0.048130	3.603242
243.404322	4369.324767	16.547981	-0.048159	3.600129
243.229886	4361.348795	16.552986	-0.048121	3.597001
243.025947	4353.374004	16.557991	-0.048078	3.593870
242.858621	4345.335208	16.562995	-0.048042	3.590711
242.980396	4337.333533	16.568000	-0.048059	3.587573
242.902817	4329.342143	16.573005	-0.048040	3.584431
242.669528	4321.377054	16.578010	-0.047991	3.581291
242.744786	4313.409258	16.583015	-0.048000	3.578157
242.702633	4305.356408	16.588019	-0.047987	3.574982
242.472388	4297.382282	16.593024	-0.047939	3.571831
242.597723	4289.366254	16.598029	-0.047957	3.568671
242.497589	4281.366774	16.603034	-0.047933	3.565508
242.526454	4273.413058	16.608039	-0.047933	3.562363
242.600788	4265.387295	16.613043	-0.047942	3.559189
242.497696	4257.417284	16.618048	-0.047917	3.556029
242.535296	4249.347914	16.623053	-0.047919	3.552831
242.255068	4241.290642	16.628058	-0.047862	3.549625
242.597300	4233.334063	16.633063	-0.047920	3.546475
242.451300	4225.370000	16.638067	-0.047888	3.543305
242.259580	4217.392262	16.643072	-0.047847	3.540125
242.277378	4209.463973	16.648077	-0.047845	3.536968
242.234879	4201.412665	16.653082	-0.047832	3.533757
242.201490	4193.415721	16.658087	-0.047821	3.530565
241.921093	4185.444011	16.663091	-0.047763	3.527374
241.997228	4177.435320	16.668096	-0.047772	3.524175
242.025790	4169.463244	16.673101	-0.047772	3.520986
241.752825	4161.486395	16.678106	-0.047716	3.517784
241.671117	4153.492141	16.683111	-0.047696	3.514577
241.710581	4145.474122	16.688115	-0.047698	3.511362
241.703963	4137.440565	16.693120	-0.047692	3.508136
241.795089	4129.437906	16.698125	-0.047703	3.504922
241.811806	4121.459178	16.703130	-0.047701	3.501713
241.935226	4113.488771	16.708135	-0.047719	3.498508
241.624464	4105.532340	16.713139	-0.047656	3.495291
241.676164	4097.506336	16.718144	-0.047661	3.492056
241.708970	4089.519376	16.723149	-0.047662	3.488832
241.411156	4081.516317	16.728154	-0.047601	3.485588
241.628937	4073.569772	16.733159	-0.047636	3.482380
241.304547	4065.569937	16.738163	-0.047571	3.479131
241.300260	4057.581683	16.743168	-0.047565	3.475894
241.361724	4049.565665	16.748173	-0.047571	3.472644
241.342125	4041.513612	16.753178	-0.047562	3.469374
241.427030	4033.551446	16.758183	-0.047573	3.466141
241.308679	4025.562272	16.763187	-0.047545	3.462887
241.339952	4017.556430	16.768192	-0.047546	3.459628
241.268198	4009.637594	16.773197	-0.047528	3.456399
241.122312	4001.566165	16.778202	-0.047495	3.453101
241.199150	3993.596141	16.783207	-0.047504	3.449849
240.973766	3985.640461	16.788211	-0.047457	3.446590
241.040519	3977.610020	16.793216	-0.047464	3.443307
240.972571	3969.651491	16.798221	-0.047446	3.440046
240.927661	3961.637765	16.803226	-0.047433	3.436760
241.040946	3953.636319	16.808231	-0.047449	3.433481
240.949335	3945.604514	16.813235	-0.047427	3.430179
240.951892	3937.629704	16.818240	-0.047422	3.426901
241.070477	3929.648447	16.823245	-0.047439	3.423621
240.860530	3921.660928	16.828250	-0.047394	3.420324
240.861365	3913.713772	16.833255	-0.047389	3.417048
240.811782	3905.710355	16.838259	-0.047375	3.413744
240.479626	3897.706418	16.843264	-0.047308	3.410426
240.498050	3889.696384	16.848269	-0.047306	3.407115
240.443089	3881.717589	16.853274	-0.047291	3.403811
240.488516	3873.754760	16.858279	-0.047294	3.400514
240.528492	3865.754941	16.863283	-0.047296	3.397198
240.351456	3857.743536	16.868288	-0.047258	3.393866
240.485495	3849.665861	16.873293	-0.047278	3.390515
240.343750	3841.698890	16.878298	-0.047246	3.387197
240.333447	3833.745184	16.883303	-0.047239	3.383885
240.420261	3825.769335	16.888307	-0.047250	3.380564
240.177869	3817.770123	16.893312	-0.047200	3.377219
240.314797	3809.787798	16.898317	-0.047220	3.373891
240.164189	3801.763139	16.903322	-0.047187	3.370532
240.318399	3793.790624	16.908327	-0.047210	3.367202
240.143594	3785.822806	16.913331	-0.047173	3.363859
240.052482	3777.843158	16.918336	-0.047150	3.360511
240.147160	3769.873377	16.923341	-0.047163	3.357170
239.900014	3761.862954	16.928346	-0.047112	3.353796
239.998937	3753.818194	16.933351	-0.047125	3.350417
239.964765	3745.835293	16.938355	-0.047113	3.347056
239.915697	3737.834320	16.943360	-0.047099	3.343683
239.796058	3729.898639	16.948365	-0.047072	3.340332
239.758718	3721.892849	16.953370	-0.047059	3.336951
239.786986	3713.885033	16.958375	-0.047059	3.333568
239.620209	3705.876598	16.963379	-0.047023	3.330174
239.693211	3697.879685	16.968384	-0.047032	3.326790
239.822892	3689.909450	16.973389	-0.047051	3.323417
239.765057	3681.905683	16.978394	-0.047035	3.320019
239.624452	3673.994591	16.983399	-0.047003	3.316653
239.683582	3665.949156	16.988403	-0.047009	3.313234
239.512303	3657.909716	16.993408	-0.046972	3.309806
239.469923	3649.951453	16.998413	-0.046959	3.306414
239.279738	3641.969193	17.003418	-0.046918	3.303002
239.430205	3633.980933	17.008423	-0.046941	3.299597
239.280746	3626.024772	17.013427	-0.046908	3.296191
239.092139	3618.025721	17.018432	-0.046868	3.292762
239.314443	3609.999622	17.023437	-0.046904	3.289333
239.025526	3602.044577	17.028442	-0.046845	3.285911
239.097243	3594.070497	17.033447	-0.046853	3.282491
239.209263	3586.071271	17.038451	-0.046869	3.279059
239.209231	3578.072391	17.043456	-0.046864	3.275619
239.206043	3570.077131	17.048461	-0.046858	3.272177
239.120614	3562.045649	17.053466	-0.046837	3.268712
239.097396	3554.084313	17.058471	-0.046827	3.265276
238.967288	3546.100686	17.063475	-0.046798	3.261823
238.823848	3538.123914	17.068480	-0.046766	3.258368
238.987899	3530.131769	17.073485	-0.046791	3.254916
239.028709	3522.118318	17.078490	-0.046794	3.251445
238.955850	3514.133238	17.083495	-0.046775	3.247979
239.007526	3506.121501	17.088499	-0.046779	3.244502
238.782439	3498.193487	17.093504	-0.046732	3.241047
238.667943	3490.232943	17.098509	-0.046706	3.237579
238.582025	3482.213865	17.103514	-0.046685	3.234082
238.654126	3474.145135	17.108519	-0.046693	3.230566
238.659223	3466.140731	17.113523	-0.046688	3.227072
238.569744	3458.150989	17.118528	-0.046667	3.223577
238.566185	3450.216822	17.123533	-0.046661	3.220105
238.500083	3442.232260	17.128538	-0.046643	3.216606
238.561052	3434.245174	17.133543	-0.046649	3.213106
238.322887	3426.235975	17.138547	-0.046600	3.209581
238.282897	3418.268802	17.143552	-0.046587	3.206078
238.176498	3410.315230	17.148557	-0.046562	3.202575
238.147302	3402.325536	17.153562	-0.046552	3.199055
238.299878	3394.325952	17.158567	-0.046575	3.195535
238.184424	3386.317527	17.163571	-0.046548	3.191995
237.974358	3378.334140	17.168576	-0.046504	3.188459
238.050633	3370.330204	17.173581	-0.046513	3.184922
237.993560	3362.363411	17.178586	-0.046497	3.181392
237.969102	3354.374911	17.183591	-0.046487	3.177849
238.014456	3346.387911	17.188595	-0.046491	3.174306
237.908765	3338.374516	17.193600	-0.046466	3.170741
237.828597	3330.404198	17.198605	-0.046446	3.167192
237.737844	3322.396936	17.203610	-0.046423	3.163623
237.735997	3314.452424	17.208615	-0.046418	3.160081
237.680078	3306.492717	17.213619	-0.046402	3.156526
237.454729	3298.482397	17.218624	-0.046355	3.152937
237.672784	3290.427571	17.223629	-0.046391	3.149343
237.577106	3282.450139	17.228634	-0.046368	3.145766
237.696380	3274.473990	17.233639	-0.046385	3.142195
237.593910	3266.520978	17.238643	-0.046360	3.138621
237.349109	3258.514010	17.243648	-0.046310	3.135012
237.438141	3250.510529	17.248653	-0.046321	3.131415
237.266320	3242.521184	17.253658	-0.046284	3.127809
237.327310	3234.550623	17.258663	-0.046290	3.124217
237.394882	3226.578181	17.263667	-0.046297	3.120621
237.254359	3218.636261	17.268672	-0.046266	3.117025
237.317719	3210.624674	17.273677	-0.046273	3.113402
237.331874	3202.584589	17.278682	-0.046270	3.109761
237.290372	3194.615201	17.283687	-0.046257	3.106144
237.244532	3186.634938	17.288691	-0.046243	3.102518
237.345604	3178.642430	17.293696	-0.046257	3.098889
237.097642	3170.692944	17.298701	-0.046206	3.095260
236.784367	3162.706080	17.303706	-0.046142	3.091606
236.825068	3154.701314	17.308711	-0.046145	3.087955
237.044717	3146.662634	17.313715	-0.046180	3.084294
236.938634	3138.738699	17.318720	-0.046155	3.080665
236.764538	3130.792896	17.323725	-0.046118	3.077019
236.836459	3122.715882	17.328730	-0.046126	3.073319
236.555892	3114.695339	17.333735	-0.046068	3.069625
236.601333	3106.713795	17.338739	-0.046072	3.065960
236.583114	3098.753710	17.343744	-0.046063	3.062297
236.562809	3090.798633	17.348749	-0.046054	3.058631
236.343986	3082.802438	17.353754	-0.046008	3.054933
236.588673	3074.803521	17.358759	-0.046049	3.051252
236.738595	3066.828621	17.363763	-0.046071	3.047572
236.433888	3058.863685	17.368768	-0.046009	3.043871
236.257759	3050.900013	17.373773	-0.045971	3.040172
236.374018	3042.924579	17.378778	-0.045988	3.036477
236.461746	3034.912054	17.383783	-0.045999	3.032759
236.286334	3026.923256	17.388787	-0.045961	3.029035
236.190494	3018.924697	17.393792	-0.045938	3.025305
236.239240	3010.979180	17.398797	-0.045942	3.021603
236.007225	3003.001889	17.403802	-0.045894	3.017867
235.993559	2995.021070	17.408807	-0.045886	3.014136
235.968306	2986.990024	17.413811	-0.045876	3.010376
235.929108	2978.991133	17.418816	-0.045863	3.006626
236.100670	2971.031251	17.423821	-0.045890	3.002900
235.939536	2963.079738	17.428826	-0.045855	2.999157
235.817369	2955.110237	17.433831	-0.045827	2.995402
235.729054	2947.094869	17.438835	-0.045806	2.991623
235.685938	2939.077604	17.443840	-0.045792	2.987841
235.783499	2931.092569	17.448845	-0.045805	2.984075
235.664508	2923.136662	17.453850	-0.045778	2.980308
235.444490	2915.212201	17.458855	-0.045732	2.976546
235.642580	2907.165634	17.463859	-0.045763	2.972743
235.551276	2899.173397	17.468864	-0.045741	2.968946
235.730249	2891.199216	17.473869	-0.045769	2.965166
235.533356	2883.247298	17.478874	-0.045728	2.961372
235.510506	2875.263360	17.483879	-0.045718	2.957568
235.546477	2867.277478	17.488883	-0.045720	2.953761
235.414242	2859.257986	17.493888	-0.045690	2.949924
235.323674	2851.332565	17.498893	-0.045668	2.946129
235.180227	2843.335175	17.503898	-0.045636	2.942292
235.211097	2835.354740	17.508903	-0.045636	2.938467
235.066570	2827.381667	17.513907	-0.045604	2.934632
234.925455	2819.369399	17.518912	-0.045573	2.930773
235.034935	2811.392250	17.523917	-0.045588	2.926939
234.970265	2803.410238	17.528922	-0.045571	2.923088
235.037339	2795.437919	17.533927	-0.045578	2.919244
235.044572	2787.474242	17.538931	-0.045574	2.915396
234.882321	2779.392713	17.543936	-0.045539	2.911476
234.920141	2771.410216	17.548941	-0.045541	2.907610
234.732828	2763.438081	17.553946	-0.045501	2.903732
234.771781	2755.483793	17.558951	-0.045503	2.899870
234.801335	2747.527657	17.563955	-0.045503	2.896001
234.650353	2739.534919	17.568960	-0.045470	2.892099
234.351817	2731.603340	17.573965	-0.045409	2.888213
234.526953	2723.565362	17.578970	-0.045436	2.884296
234.453043	2715.633588	17.583975	-0.045417	2.880413
234.346780	2707.663934	17.588979	-0.045393	2.876503
234.337547	2699.644064	17.593984	-0.045386	2.872569
234.447182	2691.659976	17.598989	-0.045401	2.868654
234.256130	2683.678621	17.603994	-0.045360	2.864718
234.329517	2675.736245	17.608999	-0.045369	2.860811
234.184613	2667.766011	17.614003	-0.045336	2.856872
234.101575	2659.762593	17.619008	-0.045316	2.852915
234.255911	2651.746645	17.624013	-0.045339	2.848959
234.174965	2643.774058	17.629018	-0.045319	2.845006
234.103515	2635.842973	17.634023	-0.045301	2.841069
233.994562	2627.885719	17.639027	-0.045275	2.837111
234.011927	2619.849341	17.644032	-0.045273	2.833116
233.997831	2611.864212	17.649037	-0.045265	2.829138
234.026660	2603.860394	17.654042	-0.045265	2.825149
233.928842	2595.917963	17.659047	-0.045242	2.821176
233.811256	2587.964706	17.664051	-0.045215	2.817192
233.793523	2579.955863	17.669056	-0.045206	2.813180
233.769801	2571.989001	17.674061	-0.045197	2.809183
233.592631	2564.030664	17.679066	-0.045159	2.805176
233.684148	2556.050941	17.684071	-0.045171	2.801167
233.571961	2548.096835	17.689075	-0.045145	2.797154
233.491415	2540.084986	17.694080	-0.045124	2.793108
233.573154	2532.077091	17.699085	-0.045134	2.789068
233.452872	2524.107914	17.704090	-0.045107	2.785029
233.444182	2516.150314	17.709095	-0.045100	2.780997
233.349591	2508.198894	17.714099	-0.045077	2.776957
233.330686	2500.202987	17.719104	-0.045068	2.772893
233.456510	2492.204345	17.724109	-0.045087	2.768830
233.223246	2484.247173	17.729114	-0.045038	2.764762
233.177347	2476.291484	17.734119	-0.045024	2.760699
233.117392	2468.332091	17.739123	-0.045008	2.756627
232.969962	2460.282642	17.744128	-0.044975	2.752498
233.088786	2452.263264	17.749133	-0.044992	2.748394
233.060683	2444.282863	17.754138	-0.044982	2.744295
232.892321	2436.367996	17.759143	-0.044945	2.740215
232.842792	2428.431547	17.764147	-0.044931	2.736125
232.760118	2420.421396	17.769152	-0.044910	2.731989
232.784456	2412.443319	17.774157	-0.044910	2.727870
232.739334	2404.460215	17.779162	-0.044896	2.723738
232.703046	2396.505660	17.784167	-0.044884	2.719615
232.587433	2388.579873	17.789171	-0.044858	2.715495
232.554550	2380.535615	17.794176	-0.044846	2.711313
232.745844	2372.551857	17.799181	-0.044877	2.707170
232.640149	2364.599685	17.804186	-0.044852	2.703018
232.495377	2356.636399	17.809191	-0.044820	2.698852
232.527301	2348.676750	17.814195	-0.044820	2.694692
232.420206	2340.675242	17.819200	-0.044795	2.690495
232.357011	2332.728559	17.824205	-0.044778	2.686323
232.159906	2324.777195	17.829210	-0.044736	2.682134
232.434361	2316.776497	17.834215	-0.044782	2.677942
232.214343	2308.822113	17.839219	-0.044736	2.673736
232.036000	2300.794921	17.844224	-0.044698	2.669488
232.197934	2292.823575	17.849229	-0.044723	2.665285
232.104408	2284.867571	17.854234	-0.044700	2.661066
231.937560	2276.916715	17.859239	-0.044664	2.656839
231.921075	2268.933203	17.864243	-0.044656	2.652597
231.909241	2260.945478	17.869248	-0.044648	2.648347
232.024416	2252.972853	17.874253	-0.044665	2.644106
231.796837	2245.030516	17.879258	-0.044617	2.639852
231.700991	2237.086066	17.884263	-0.044594	2.635599
231.780138	2229.070003	17.889267	-0.044604	2.631312
231.818645	2221.078369	17.894272	-0.044606	2.627029
231.805019	2213.131159	17.899277	-0.044598	2.622758
231.654586	2205.168617	17.904282	-0.044565	2.618464
231.379457	2197.226297	17.909287	-0.044508	2.614165
231.380722	2189.231374	17.914291	-0.044503	2.609849
231.409856	2181.252839	17.919296	-0.044504	2.605537
231.415909	2173.304477	17.924301	-0.044499	2.601232
231.233991	2165.355351	17.929306	-0.044460	2.596907
231.143795	2157.278673	17.934311	-0.044438	2.592511
231.178062	2149.218497	17.939315	-0.044440	2.588126
231.181849	2141.251288	17.944320	-0.044435	2.583782
231.269201	2133.353797	17.949325	-0.044446	2.579474
231.116029	2125.417876	17.954330	-0.044412	2.575121
230.945581	2117.447835	17.959335	-0.044376	2.570741
230.981070	2109.472598	17.964339	-0.044377	2.566365
230.946812	2101.521734	17.969344	-0.044365	2.561991
231.134945	2093.565387	17.974349	-0.044395	2.557621
230.955750	2085.601801	17.979354	-0.044357	2.553214
230.791067	2077.638941	17.984359	-0.044321	2.548800
230.733464	2069.673821	17.989363	-0.044305	2.544386
230.676028	2061.713536	17.994368	-0.044289	2.539966
230.714821	2053.759919	17.999373	-0.044291	2.535549
230.606409	2045.782611	18.004378	-0.044266	2.531101
230.550478	2037.811557	18.009383	-0.044250	2.526652
230.442136	2029.866866	18.014387	-0.044225	2.522206
230.363574	2021.916817	18.019392	-0.044205	2.517752
230.348551	2013.942114	18.024397	-0.044197	2.513280
230.287719	2005.926405	18.029402	-0.044181	2.508774
230.253244	1997.962759	18.034407	-0.044169	2.504291
230.176500	1990.039872	18.039411	-0.044150	2.499820
230.052015	1982.066382	18.044416	-0.044121	2.495309
230.225743	1974.071544	18.049421	-0.044148	2.490800
230.153781	1966.114658	18.054426	-0.044130	2.486285
230.090620	1958.173043	18.059431	-0.044113	2.481772
230.042383	1950.226690	18.064435	-0.044099	2.477249
229.970594	1942.242924	18.069440	-0.044080	2.472695
229.966605	1934.259327	18.074445	-0.044074	2.468137
229.819313	1926.320093	18.079450	-0.044042	2.463586
229.691354	1918.366412	18.084455	-0.044013	2.459019
229.756789	1910.405784	18.089459	-0.044020	2.454454
229.585377	1902.434032	18.094464	-0.043983	2.449857
229.671459	1894.450292	18.099469	-0.043993	2.445263
229.757480	1886.506354	18.104474	-0.044004	2.440684
229.626581	1878.576715	18.109479	-0.043975	2.436088
229.687695	1870.540702	18.114483	-0.043981	2.431436
229.302907	1862.588870	18.119488	-0.043904	2.426790
229.527050	1854.613494	18.124493	-0.043941	2.422169
229.302953	1846.694384	18.129498	-0.043894	2.417536
229.215273	1838.722276	18.134503	-0.043872	2.412874
229.290370	1830.755720	18.139507	-0.043881	2.408219
229.264524	1822.781761	18.144512	-0.043871	2.403543
229.215051	1814.859136	18.149517	-0.043857	2.398886
229.050727	1806.920871	18.154522	-0.043821	2.394202
228.961944	1798.934450	18.159527	-0.043799	2.389486
228.953329	1790.977663	18.164531	-0.043792	2.384785
229.113462	1782.997084	18.169536	-0.043817	2.380073
229.119952	1775.065964	18.174541	-0.043813	2.375370
228.994984	1767.103660	18.179546	-0.043785	2.370628
228.772833	1759.159966	18.184551	-0.043738	2.365879
228.826152	1751.217696	18.189555	-0.043743	2.361145
228.670370	1743.263986	18.194560	-0.043709	2.356377
228.679299	1735.279993	18.199565	-0.043705	2.351594
228.444198	1727.330977	18.204570	-0.043656	2.346803
228.410224	1719.351370	18.209575	-0.043645	2.342000
228.375858	1711.424155	18.214579	-0.043633	2.337218
228.247768	1703.470413	18.219584	-0.043604	2.332403
228.531279	1695.464504	18.224589	-0.043652	2.327581
228.453798	1687.535005	18.229594	-0.043632	2.322765
228.170896	1679.612839	18.234599	-0.043574	2.317926
228.245358	1671.663139	18.239603	-0.043583	2.313090
228.144629	1663.683988	18.244608	-0.043559	2.308212
228.206125	1655.733425	18.249613	-0.043565	2.303354
228.130362	1647.791971	18.254618	-0.043546	2.298480
227.939204	1639.855851	18.259623	-0.043505	2.293589
227.848266	1631.893846	18.264627	-0.043483	2.288680
227.822094	1623.930689	18.269632	-0.043473	2.283765
228.000938	1615.993449	18.274637	-0.043501	2.278874
227.899447	1608.037632	18.279642	-0.043477	2.273936
227.735492	1600.031205	18.284647	-0.043442	2.268951
227.767341	1592.070453	18.289651	-0.043442	2.264000
227.721868	1584.135316	18.294656	-0.043429	2.259047
227.660751	1576.208546	18.299661	-0.043412	2.254087
227.727289	1568.224721	18.304666	-0.043419	2.249092
227.693278	1560.278305	18.309671	-0.043408	2.244101
227.648230	1552.371440	18.314675	-0.043394	2.239122
227.343977	1544.441763	18.319680	-0.043333	2.234095
227.421445	1536.471267	18.324685	-0.043342	2.229064
227.432641	1528.520600	18.329690	-0.043339	2.224029
227.270277	1520.598527	18.334695	-0.043303	2.218985
227.341000	1512.646610	18.339699	-0.043311	2.213931
227.390429	1504.670799	18.344704	-0.043315	2.208848
227.347731	1496.743598	18.349709	-0.043302	2.203777
227.000301	1488.859419	18.354714	-0.043232	2.198694
227.090935	1480.877164	18.359719	-0.043244	2.193576
226.931588	1472.931640	18.364723	-0.043209	2.188446
226.930602	1464.958477	18.369728	-0.043204	2.183302
227.103008	1457.019260	18.374733	-0.043231	2.178183
227.200688	1449.060124	18.379738	-0.043244	2.173032
226.845365	1441.140565	18.384743	-0.043173	2.167853
226.663231	1433.245892	18.389747	-0.043134	2.162693
226.719852	1425.288589	18.394752	-0.043139	2.157503
226.523929	1417.373833	18.399757	-0.043097	2.152304
226.410352	1409.412841	18.404762	-0.043071	2.147070
226.354610	1401.469915	18.409767	-0.043055	2.141840
226.343738	1393.544230	18.414771	-0.043048	2.136614
226.015177	1385.605720	18.419776	-0.042982	2.131335
226.225075	1377.643533	18.424781	-0.043016	2.126080
226.142959	1369.720854	18.429786	-0.042995	2.120809
225.930612	1361.809299	18.434791	-0.042951	2.115521
225.980377	1353.804616	18.439795	-0.042955	2.110182
225.881663	1345.845098	18.444800	-0.042931	2.104845
226.005766	1337.918866	18.449805	-0.042949	2.099539
225.748623	1330.025187	18.454810	-0.042896	2.094204
225.966769	1322.026852	18.459815	-0.042932	2.088831
225.895332	1314.129279	18.464819	-0.042913	2.083485
225.564871	1306.243489	18.469824	-0.042846	2.078107
225.872848	1298.261204	18.474829	-0.042899	2.072712
225.680620	1290.346133	18.479834	-0.042858	2.067300
225.475057	1282.453408	18.484839	-0.042814	2.061887
225.480806	1274.516940	18.489843	-0.042810	2.056451
225.584647	1266.549151	18.494848	-0.042824	2.050989
225.517968	1258.628406	18.499853	-0.042807	2.045528
225.096638	1250.772586	18.504858	-0.042723	2.040061
225.158251	1242.811027	18.509863	-0.042730	2.034555
225.161827	1234.859285	18.514867	-0.042725	2.029035
224.988863	1226.934589	18.519872	-0.042688	2.023500
225.101705	1219.003325	18.524877	-0.042703	2.017975
225.147192	1211.060866	18.529882	-0.042707	2.012421
224.930970	1203.141043	18.534887	-0.042661	2.006839
224.706226	1195.253298	18.539891	-0.042614	2.001264
224.727058	1187.322746	18.544896	-0.042613	1.995669
224.993356	1179.347077	18.549901	-0.042658	1.990052
224.695139	1171.474181	18.554906	-0.042597	1.984432
224.533567	1163.569277	18.559911	-0.042562	1.978788
224.597264	1155.633548	18.564915	-0.042568	1.973129
224.514139	1147.692361	18.569920	-0.042548	1.967435
224.466067	1139.796095	18.574925	-0.042534	1.961760
224.456644	1131.886810	18.579930	-0.042527	1.956064
224.569881	1123.891716	18.584935	-0.042543	1.950302
224.567353	1115.977102	18.589939	-0.042537	1.944569
224.308614	1108.094069	18.594944	-0.042484	1.938814
224.315387	1100.175617	18.599949	-0.042480	1.933045
224.170552	1092.256699	18.604954	-0.042448	1.927242
223.920097	1084.368306	18.609959	-0.042396	1.921431
224.139628	1076.442047	18.614963	-0.042432	1.915628
224.082422	1068.513198	18.619968	-0.042416	1.909774
223.840836	1060.631972	18.624973	-0.042366	1.903917
223.903216	1052.717092	18.629978	-0.042372	1.898050
223.863989	1044.793866	18.634983	-0.042360	1.892148
223.754187	1036.891899	18.639987	-0.042334	1.886236
223.826111	1028.978568	18.644992	-0.042342	1.880316
223.852801	1021.080775	18.649997	-0.042342	1.874385
223.474851	1013.196286	18.655002	-0.042267	1.868398
223.419103	1005.266272	18.660007	-0.042251	1.862395
223.531268	997.364287	18.665011	-0.042267	1.856413
223.356063	989.458156	18.670016	-0.042229	1.850375
223.287228	981.565914	18.675021	-0.042211	1.844340
223.192189	973.686666	18.680026	-0.042189	1.838293
223.116453	965.778721	18.685031	-0.042169	1.832205
223.002522	957.885184	18.690035	-0.042143	1.826104
223.070504	949.960439	18.695040	-0.042150	1.819980
223.029336	942.078912	18.700045	-0.042138	1.813856
222.835035	934.194857	18.705050	-0.042096	1.807690
222.852783	926.284488	18.710055	-0.042094	1.801509
222.963005	918.394630	18.715059	-0.042110	1.795333
222.828919	910.443563	18.720064	-0.042080	1.789058
222.827884	902.548138	18.725069	-0.042074	1.782822
222.587753	894.703911	18.730074	-0.042025	1.776574
222.573093	886.797695	18.735079	-0.042017	1.770283
222.576123	878.915621	18.740083	-0.042012	1.763991
222.241948	871.073016	18.745088	-0.041945	1.757666
222.280503	863.172563	18.750093	-0.041947	1.751319
222.211001	855.276253	18.755098	-0.041929	1.744938
222.010768	847.428938	18.760103	-0.041886	1.738556
222.167040	839.507320	18.765107	-0.041910	1.732136
222.210333	831.603967	18.770112	-0.041913	1.725693
222.143700	823.756260	18.775117	-0.041896	1.719257
222.049310	815.886032	18.780122	-0.041873	1.712775
222.044275	807.980579	18.785127	-0.041867	1.706250
221.775912	800.148743	18.790131	-0.041812	1.699727
221.575921	792.292165	18.795136	-0.041770	1.693167
221.669803	784.385169	18.800141	-0.041782	1.686579
221.631647	776.522578	18.805146	-0.041770	1.679984
221.524282	768.665522	18.810151	-0.041745	1.673359
221.526071	760.790031	18.815155	-0.041740	1.666706
221.391832	752.924192	18.820160	-0.041710	1.660016
221.417386	745.062879	18.825165	-0.041709	1.653325
221.453500	737.174774	18.830170	-0.041711	1.646585
221.448671	729.322672	18.835175	-0.041705	1.639843
221.303375	721.483131	18.840179	-0.041673	1.633065
221.175873	713.570996	18.845184	-0.041644	1.626198
221.275003	705.710182	18.850189	-0.041657	1.619377
221.042347	697.897478	18.855194	-0.041609	1.612524
221.040818	690.015704	18.860199	-0.041604	1.605613
220.957156	682.205398	18.865203	-0.041583	1.598724
221.005716	674.335476	18.870208	-0.041587	1.591771
220.609556	666.537579	18.875213	-0.041508	1.584787
220.540782	658.706443	18.880218	-0.041490	1.577790
220.567728	650.821776	18.885223	-0.041490	1.570728
220.554490	642.999543	18.890227	-0.041482	1.563684
220.442866	635.172949	18.895232	-0.041457	1.556590
220.188093	627.350230	18.900237	-0.041404	1.549446
220.224808	619.492639	18.905242	-0.041406	1.542280
219.957014	611.688944	18.910247	-0.041351	1.535085
220.206408	603.808583	18.915251	-0.041392	1.527863
220.053682	595.999923	18.920256	-0.041359	1.520612
219.790215	588.221185	18.925261	-0.041305	1.513337
219.702550	580.386741	18.930266	-0.041283	1.506002
219.750500	572.549097	18.935271	-0.041287	1.498649
219.783059	564.718626	18.940275	-0.041288	1.491264
219.561953	556.929088	18.945280	-0.041242	1.483841
219.535775	549.125027	18.950285	-0.041232	1.476398
219.516595	541.259967	18.955290	-0.041223	1.468860
219.407171	533.452450	18.960295	-0.041198	1.461324
219.568514	525.638946	18.965299	-0.041223	1.453786
219.442138	517.835421	18.970304	-0.041194	1.446173
219.120165	510.103042	18.975309	-0.041129	1.438557
219.006828	502.316688	18.980314	-0.041103	1.430881
219.011665	494.502553	18.985319	-0.041099	1.423156
218.990235	486.726455	18.990323	-0.041090	1.415422
218.824835	478.942159	18.995328	-0.041054	1.407614
218.733096	471.171595	19.000333	-0.041032	1.399788
218.750604	463.382159	19.005338	-0.041030	1.391917
218.676208	455.593101	19.010343	-0.041011	1.383986
218.462938	447.855310	19.015347	-0.040966	1.376039
218.491811	440.063639	19.020352	-0.040966	1.368031
218.577514	432.289285	19.025357	-0.040977	1.360004
218.485391	424.545975	19.030362	-0.040955	1.351931
218.222897	416.811207	19.035367	-0.040901	1.343788
218.311578	409.050181	19.040371	-0.040913	1.335630
217.948815	401.340220	19.045376	-0.040840	1.327395
218.194933	393.561227	19.050381	-0.040881	1.319144
218.152819	385.744257	19.055386	-0.040868	1.310749
217.815898	378.001145	19.060391	-0.040800	1.302326
217.797349	370.285258	19.065395	-0.040792	1.293936
217.632266	362.567650	19.070400	-0.040756	1.285462
217.597778	354.869598	19.075405	-0.040745	1.276977
217.368683	347.177118	19.080410	-0.040697	1.268406
217.314051	339.467400	19.085415	-0.040682	1.259790
217.278359	331.765390	19.090419	-0.040670	1.251127
217.053972	324.089984	19.095424	-0.040623	1.242397
217.043653	316.399303	19.100429	-0.040616	1.233630
217.044383	308.684141	19.105434	-0.040612	1.224773
216.601248	301.062705	19.110439	-0.040524	1.215874
216.663862	293.361575	19.115443	-0.040531	1.206916
216.696538	285.677207	19.120448	-0.040532	1.197904
216.734455	278.000303	19.125453	-0.040534	1.188835
216.507112	270.379762	19.130458	-0.040487	1.179709
216.476993	262.717127	19.135463	-0.040476	1.170501
216.576295	255.058104	19.140467	-0.040490	1.161252
216.242633	247.465601	19.145472	-0.040423	1.151919
216.075108	239.827940	19.150477	-0.040386	1.142489
215.978458	232.214450	19.155482	-0.040363	1.133026
215.660450	224.632872	19.160487	-0.040299	1.123476
215.602665	217.041574	19.165491	-0.040284	1.113888
215.456896	209.442035	19.170496	-0.040251	1.104186
215.493054	201.840811	19.175501	-0.040253	1.094437
215.606456	194.232667	19.180506	-0.040269	1.084608
215.478208	186.683181	19.185511	-0.040241	1.074712
215.298119	179.139849	19.190515	-0.040202	1.064720
215.036404	171.620502	19.195520	-0.040149	1.054647
214.902080	164.092874	19.200525	-0.040119	1.044495
214.912180	156.560105	19.205530	-0.040116	1.034270
214.640604	149.069994	19.210535	-0.040060	1.023935
214.737963	141.546641	19.215539	-0.040073	1.013537
214.674107	134.050685	19.220544	-0.040057	1.003030
214.654210	126.566654	19.225549	-0.040048	0.992440
214.452144	119.097036	19.230554	-0.040006	0.981711
213.928060	111.721370	19.235559	-0.039903	0.970918
214.133189	104.235013	19.240563	-0.039937	0.960028
213.981347	96.820907	19.245568	-0.039904	0.949027
213.633435	89.463836	19.250573	-0.039834	0.937932
213.714339	82.042243	19.255578	-0.039844	0.926720
213.537219	74.694750	19.260583	-0.039806	0.915415
213.439878	67.330941	19.265587	-0.039784	0.903965
213.207475	60.246820	19.270592	-0.039736	0.892772