Fri Mar 12 12:15:47 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.696971	0.072118	0.000000	0.000010	0.721116
0.763597	0.011648	0.005005	-0.000002	0.721020
0.603080	-0.035459	0.010010	0.000028	0.720871
0.618119	-0.035406	0.015014	0.000025	0.720876
0.733339	-0.056325	0.020019	0.000004	0.720876
0.660303	-0.045030	0.025024	0.000017	0.720872
0.737224	-0.054647	0.030029	0.000003	0.720880
0.666346	-0.045005	0.035034	0.000016	0.720875
0.615730	-0.034846	0.040038	0.000025	0.720877
0.860615	-0.077150	0.045043	-0.000020	0.720879
0.731978	-0.057104	0.050048	0.000004	0.720874
0.856467	-0.075668	0.055053	-0.000019	0.720881
0.909567	-0.088857	0.060058	-0.000029	0.720874
1.044137	-0.110446	0.065062	-0.000054	0.720878
0.939356	-0.092784	0.070067	-0.000035	0.720876
0.857930	-0.135876	0.075072	-0.000020	0.720763
0.875404	-0.250256	0.080077	-0.000023	0.720544
0.712547	-0.225858	0.085082	0.000007	0.720535
0.610469	-0.206932	0.090086	0.000026	0.720536
0.706944	-0.223086	0.095091	0.000009	0.720538
0.671449	-0.219030	0.100096	0.000015	0.720534
0.818225	-0.241843	0.105101	-0.000012	0.720540
0.710908	-0.347361	0.110106	0.000008	0.720295
0.791102	-0.398464	0.115110	-0.000007	0.720223
0.606898	-0.365902	0.120115	0.000027	0.720222
0.806359	-0.403965	0.125120	-0.000010	0.720217
1.032618	-0.438873	0.130125	-0.000052	0.720228
0.895631	-0.559495	0.135130	-0.000026	0.719942
0.844487	-0.573445	0.140134	-0.000017	0.719897
0.767971	-0.558715	0.145139	-0.000003	0.719899
0.770062	-0.562419	0.150144	-0.000003	0.719892
0.750058	-0.661556	0.155149	0.000001	0.719690
0.638785	-0.690328	0.160154	0.000021	0.719594
0.935813	-0.739549	0.165158	-0.000034	0.719601
0.603177	-0.679562	0.170163	0.000028	0.719603
0.526018	-0.834654	0.175168	0.000043	0.719270
0.466146	-0.821344	0.180173	0.000054	0.719275
0.585746	-0.847517	0.185178	0.000031	0.719266
0.617856	-0.931196	0.190182	0.000025	0.719112
0.367929	-0.964113	0.195187	0.000072	0.718959
0.340956	-0.961094	0.200192	0.000077	0.718956
0.532716	-1.026501	0.205197	0.000041	0.718894
0.595928	-1.168588	0.210202	0.000030	0.718636
0.580475	-1.162796	0.215206	0.000033	0.718642
0.534715	-1.194665	0.220211	0.000041	0.718563
0.553417	-1.307224	0.225216	0.000038	0.718347
0.807933	-1.348489	0.230221	-0.000010	0.718355
0.658775	-1.422505	0.235226	0.000018	0.718157
0.594541	-1.482188	0.240230	0.000030	0.718016
0.420330	-1.451125	0.245235	0.000063	0.718016
0.485496	-1.618280	0.250240	0.000051	0.717709
0.482566	-1.618947	0.255245	0.000051	0.717706
0.371727	-1.676285	0.260250	0.000072	0.717554
0.382487	-1.764265	0.265254	0.000070	0.717384
0.326408	-1.757833	0.270259	0.000080	0.717377
0.327204	-1.905059	0.275264	0.000080	0.717086
0.458481	-1.926278	0.280269	0.000056	0.717090
0.338685	-2.030233	0.285274	0.000078	0.716842
0.161946	-2.040561	0.290278	0.000111	0.716760
0.088923	-2.097316	0.295283	0.000125	0.716622
0.145446	-2.195188	0.300288	0.000114	0.716448
-0.101831	-2.184020	0.305293	0.000160	0.716383
-0.199665	-2.294085	0.310298	0.000178	0.716130
-0.188667	-2.296798	0.315302	0.000176	0.716129
-2.296473	-2.044629	0.320307	0.000569	0.715884
-2.172340	-2.070922	0.325312	0.000546	0.715876
-2.333716	-2.051356	0.330317	0.000576	0.715858
-3.421247	-2.017532	0.335322	0.000778	0.715541
-3.122936	-2.068396	0.340326	0.000723	0.715546
-3.092470	-2.072765	0.345331	0.000717	0.715548
-3.883163	-2.061721	0.350336	0.000864	0.715290
-4.112526	-2.047073	0.355341	0.000907	0.715238
-4.254221	-2.026479	0.360346	0.000933	0.715229
-4.045096	-2.086915	0.365350	0.000894	0.715183
-4.901604	-2.071664	0.370355	0.001054	0.714911
-5.256651	-2.011957	0.375360	0.001120	0.714904
-5.206194	-2.015798	0.380365	0.001110	0.714914
-5.158189	-2.028328	0.385370	0.001101	0.714906
-5.354127	-2.131368	0.390374	0.001138	0.714632
-5.962994	-2.033005	0.395379	0.001251	0.714612
-6.502186	-1.939859	0.400384	0.001352	0.714606
-5.935262	-2.038820	0.405389	0.001246	0.714610
-5.796538	-2.120853	0.410394	0.001220	0.714497
-7.061650	-2.006728	0.415398	0.001456	0.714276
-6.909068	-2.033406	0.420403	0.001427	0.714277
-7.051932	-2.009923	0.425408	0.001454	0.714273
-6.841911	-2.042669	0.430413	0.001415	0.714282
-7.001949	-2.067912	0.435418	0.001445	0.714175
-8.146386	-1.968394	0.440422	0.001658	0.713968
-7.374225	-2.103848	0.445427	0.001514	0.713972
-8.193022	-1.962726	0.450432	0.001666	0.713963
-7.942693	-2.003600	0.455437	0.001620	0.713970
-7.763043	-2.036200	0.460442	0.001586	0.713969
-8.233264	-2.072985	0.465446	0.001674	0.713729
-8.964192	-1.979589	0.470451	0.001810	0.713656
-8.986645	-1.979598	0.475456	0.001814	0.713648
-8.495398	-2.064968	0.480461	0.001723	0.713652
-8.956511	-1.985801	0.485466	0.001809	0.713646
-8.569291	-2.053186	0.490470	0.001737	0.713650
-8.484968	-2.181181	0.495475	0.001721	0.713425
-9.888286	-1.967692	0.500480	0.001982	0.713352
-9.523704	-2.027082	0.505485	0.001914	0.713363
-9.012930	-2.122369	0.510490	0.001819	0.713355
-9.409780	-2.050372	0.515494	0.001893	0.713357
-9.659135	-2.015563	0.520499	0.001939	0.713338
-10.563197	-2.015725	0.525504	0.002108	0.713018
-10.128179	-2.088690	0.530509	0.002027	0.713027
-10.699254	-1.990709	0.535514	0.002133	0.713019
-10.925635	-1.949594	0.540518	0.002175	0.713021
-10.266268	-2.065356	0.545523	0.002052	0.713024
-10.734514	-1.984206	0.550528	0.002140	0.713020
-10.676833	-2.045942	0.555533	0.002129	0.712917
-11.637262	-1.981509	0.560538	0.002308	0.712705
-11.416026	-2.020502	0.565542	0.002267	0.712706
-11.553035	-1.992410	0.570547	0.002292	0.712713
-11.790686	-1.953795	0.575552	0.002336	0.712706
-11.299930	-2.037204	0.580557	0.002245	0.712714
-11.605693	-1.986374	0.585562	0.002302	0.712706
-11.495284	-2.044586	0.590566	0.002281	0.712630
-11.910347	-2.090797	0.595571	0.002359	0.712390
-12.292532	-2.026622	0.600576	0.002430	0.712383
-12.806730	-1.929794	0.605581	0.002525	0.712393
-12.412471	-2.005104	0.610586	0.002452	0.712383
-11.804965	-2.110926	0.615590	0.002339	0.712388
-12.045537	-2.067517	0.620595	0.002384	0.712389
-12.562181	-2.081052	0.625600	0.002480	0.712178
-13.215854	-2.007160	0.630605	0.002602	0.712094
-13.341460	-1.988348	0.635610	0.002625	0.712086
-13.294331	-1.994988	0.640614	0.002616	0.712090
-13.272927	-1.997279	0.645619	0.002612	0.712093
-13.430295	-1.973747	0.650624	0.002641	0.712084
-13.353216	-1.983727	0.655629	0.002627	0.712092
-13.430049	-2.042062	0.660634	0.002641	0.711948
-14.270365	-1.987946	0.665638	0.002798	0.711757
-13.969412	-2.037663	0.670643	0.002742	0.711765
-14.455519	-1.953984	0.675648	0.002832	0.711759
-14.090362	-2.015533	0.680653	0.002764	0.711766
-13.878818	-2.054838	0.685658	0.002725	0.711763
-14.493364	-1.945220	0.690662	0.002839	0.711763
-14.268215	-2.038504	0.695667	0.002797	0.711657
-15.076296	-1.996739	0.700672	0.002948	0.711454
-14.955122	-2.014893	0.705677	0.002925	0.711460
-15.188829	-1.977518	0.710682	0.002969	0.711452
-14.913549	-2.025911	0.715686	0.002918	0.711453
-14.954457	-2.017296	0.720691	0.002925	0.711456
-15.494288	-1.924550	0.725696	0.003026	0.711449
-14.919211	-2.058138	0.730701	0.002919	0.711387
-15.791676	-2.028169	0.735706	0.003081	0.711137
-16.010216	-1.988214	0.740710	0.003122	0.711139
-15.997684	-1.990256	0.745715	0.003119	0.711139
-15.940923	-2.002644	0.750720	0.003109	0.711135
-15.765569	-2.030768	0.755725	0.003076	0.711141
-16.192747	-1.959696	0.760730	0.003156	0.711131
-15.924337	-2.020516	0.765734	0.003106	0.711105
-16.237510	-2.081166	0.770739	0.003164	0.710872
-16.962058	-1.955105	0.775744	0.003299	0.710866
-16.754989	-1.986732	0.780749	0.003260	0.710877
-16.668548	-2.006559	0.785754	0.003244	0.710868
-16.932022	-1.959143	0.790758	0.003293	0.710869
-16.544973	-2.026165	0.795763	0.003221	0.710873
-16.587129	-2.092232	0.800768	0.003229	0.710726
-17.931053	-1.949944	0.805773	0.003479	0.710532
-17.597927	-2.010603	0.810778	0.003417	0.710529
-17.460881	-2.034874	0.815782	0.003392	0.710530
-17.771146	-1.977048	0.820787	0.003450	0.710535
-17.802032	-1.976902	0.825792	0.003455	0.710524
-17.486812	-2.028275	0.830797	0.003397	0.710534
-17.326723	-2.132065	0.835802	0.003367	0.710383
-18.834837	-1.947807	0.840806	0.003648	0.710214
-18.228336	-2.054022	0.845811	0.003535	0.710218
-18.632051	-1.987236	0.850816	0.003610	0.710208
-18.479607	-2.007963	0.855821	0.003581	0.710221
-18.537290	-2.002727	0.860826	0.003592	0.710211
-18.520058	-2.003889	0.865830	0.003589	0.710214
-18.402345	-2.113916	0.870835	0.003567	0.710037
-19.890646	-1.924590	0.875840	0.003844	0.709885
-19.363023	-2.014252	0.880845	0.003746	0.709894
-19.351251	-2.017214	0.885850	0.003744	0.709892
-19.570559	-1.978721	0.890854	0.003785	0.709891
-19.282544	-2.027985	0.895859	0.003731	0.709895
-19.623067	-1.971988	0.900864	0.003794	0.709885
-19.679416	-2.003331	0.905869	0.003805	0.709803
-20.481394	-1.964268	0.910874	0.003954	0.709595
-20.255974	-2.003901	0.915878	0.003912	0.709596
-20.297911	-1.994715	0.920883	0.003920	0.709600
-20.815799	-1.906442	0.925888	0.004016	0.709591
-20.300534	-1.993945	0.930893	0.003920	0.709600
-20.227093	-2.009184	0.935898	0.003907	0.709596
-20.491735	-1.962026	0.940902	0.003956	0.709596
-20.901851	-2.045467	0.945907	0.004032	0.709283
-21.472258	-1.955163	0.950912	0.004139	0.709260
-21.570941	-1.933836	0.955917	0.004157	0.709267
-21.426933	-1.962042	0.960922	0.004130	0.709262
-21.670508	-1.916803	0.965926	0.004175	0.709266
-21.274994	-1.983826	0.970931	0.004102	0.709273
-21.607065	-1.930772	0.975936	0.004164	0.709261
-21.506003	-1.985022	0.980941	0.004145	0.709188
-22.111738	-1.993738	0.985946	0.004258	0.708955
-22.025162	-2.008355	0.990950	0.004241	0.708956
-22.209623	-1.971663	0.995955	0.004276	0.708964
-22.345959	-1.951619	1.000960	0.004301	0.708956
-22.134134	-1.986180	1.005965	0.004262	0.708962
-22.470376	-1.929611	1.010970	0.004324	0.708955
-22.167936	-2.005896	1.015974	0.004268	0.708910
-22.631836	-2.055897	1.020979	0.004354	0.708645
-23.432407	-1.918906	1.025984	0.004503	0.708633
-23.381608	-1.923250	1.030989	0.004494	0.708643
-22.706659	-2.046590	1.035994	0.004368	0.708637
-23.139213	-1.968410	1.040998	0.004449	0.708639
-23.384719	-1.920801	1.046003	0.004495	0.708647
-23.329959	-1.935788	1.051008	0.004484	0.708636
-23.091883	-2.097798	1.056013	0.004440	0.708397
-23.965009	-1.964854	1.061018	0.004603	0.708351
-23.966680	-1.965185	1.066022	0.004603	0.708350
-23.416486	-2.059824	1.071027	0.004501	0.708357
-23.805541	-1.995589	1.076032	0.004573	0.708347
-23.741845	-2.002974	1.081037	0.004561	0.708355
-23.747002	-2.087004	1.086042	0.004562	0.708184
-25.239374	-1.907456	1.091046	0.004840	0.708011
-24.588482	-2.021449	1.096051	0.004719	0.708015
-24.721718	-2.001016	1.101056	0.004743	0.708008
-24.803578	-1.981719	1.106061	0.004759	0.708018
-25.012705	-1.946864	1.111066	0.004798	0.708013
-25.193687	-1.915234	1.116070	0.004831	0.708012
-24.570646	-2.076157	1.121075	0.004715	0.707912
-25.832951	-1.959563	1.126080	0.004950	0.707694
-25.639143	-1.988820	1.131085	0.004914	0.707705
-25.644536	-1.992027	1.136090	0.004915	0.707697
-25.656528	-1.989661	1.141094	0.004917	0.707697
-25.917877	-1.940203	1.146099	0.004966	0.707703
-26.179673	-1.898682	1.151104	0.005015	0.707693
-25.679146	-1.998641	1.156109	0.004922	0.707671
-26.250470	-2.043987	1.161114	0.005028	0.707376
-26.790623	-1.948101	1.166118	0.005129	0.707375
-26.395717	-2.015579	1.171123	0.005055	0.707381
-26.564646	-1.990024	1.176128	0.005087	0.707372
-26.592047	-1.981800	1.181133	0.005092	0.707379
-26.532755	-1.994902	1.186138	0.005081	0.707373
-26.536331	-2.024295	1.191142	0.005081	0.707313
-27.408742	-1.982652	1.196147	0.005244	0.707085
-27.619586	-1.949390	1.201152	0.005283	0.707076
-27.574516	-1.953308	1.206157	0.005275	0.707084
-27.767337	-1.920770	1.211162	0.005310	0.707081
-27.821356	-1.913129	1.216166	0.005320	0.707077
-27.523949	-1.960509	1.221171	0.005265	0.707088
-27.639484	-1.945751	1.226176	0.005287	0.707076
-27.752053	-2.027148	1.231181	0.005308	0.706873
-28.686114	-1.921203	1.236186	0.005481	0.706751
-28.496958	-1.956519	1.241190	0.005446	0.706748
-28.455515	-1.959948	1.246195	0.005439	0.706756
-28.950854	-1.876903	1.251200	0.005531	0.706745
-28.035071	-2.035486	1.256205	0.005360	0.706755
-28.100772	-2.025062	1.261210	0.005373	0.706752
-28.865970	-1.969175	1.266214	0.005515	0.706590
-29.389751	-1.946941	1.271219	0.005612	0.706447
-29.216333	-1.982325	1.276224	0.005580	0.706438
-29.242098	-1.973503	1.281229	0.005585	0.706447
-29.380999	-1.951351	1.286234	0.005611	0.706442
-29.249866	-1.973449	1.291238	0.005586	0.706444
-29.075301	-2.001581	1.296243	0.005554	0.706450
-29.505503	-2.007662	1.301248	0.005634	0.706284
-30.114363	-1.974265	1.306253	0.005747	0.706133
-29.908444	-2.013112	1.311258	0.005709	0.706129
-30.320635	-1.939756	1.316262	0.005786	0.706128
-30.071289	-1.982074	1.321267	0.005739	0.706133
-29.972282	-2.004115	1.326272	0.005721	0.706124
-30.324459	-1.936411	1.331277	0.005786	0.706134
-30.378065	-2.006867	1.336282	0.005796	0.705973
-30.991793	-1.953859	1.341286	0.005911	0.705859
-30.738037	-1.994326	1.346291	0.005863	0.705869
-31.101613	-1.934254	1.351296	0.005931	0.705860
-30.938422	-1.959546	1.356301	0.005901	0.705867
-30.526182	-2.033504	1.361306	0.005824	0.705866
-31.071710	-1.938629	1.366310	0.005926	0.705861
-31.513650	-2.020208	1.371315	0.006008	0.705539
-31.892649	-1.960601	1.376320	0.006078	0.705523
-31.835723	-1.968504	1.381325	0.006068	0.705527
-31.646553	-2.003978	1.386330	0.006033	0.705524
-31.741512	-1.987636	1.391334	0.006050	0.705523
-31.829982	-1.968883	1.396339	0.006067	0.705529
-32.031668	-1.952755	1.401344	0.006104	0.705489
-32.624401	-1.984448	1.406349	0.006215	0.705212
-32.626135	-1.984338	1.411354	0.006215	0.705212
-33.088682	-1.903551	1.416358	0.006301	0.705209
-32.738168	-1.961894	1.421363	0.006236	0.705217
-32.517213	-2.005050	1.426368	0.006195	0.705209
-32.856979	-1.941653	1.431373	0.006258	0.705215
-32.981961	-1.920851	1.436378	0.006281	0.705212
-33.113052	-2.042458	1.441382	0.006306	0.704920
-33.637798	-1.963485	1.446387	0.006403	0.704891
-34.131492	-1.878692	1.451392	0.006495	0.704884
-33.419535	-2.002832	1.456397	0.006363	0.704890
-33.536096	-1.985235	1.461402	0.006384	0.704884
-33.863791	-1.926587	1.466406	0.006445	0.704884
-33.500506	-1.988760	1.471411	0.006378	0.704889
-33.976812	-2.028107	1.476416	0.006466	0.704639
-34.568664	-1.945452	1.481421	0.006577	0.704593
-34.652320	-1.931550	1.486426	0.006592	0.704591
-34.461625	-1.966597	1.491430	0.006557	0.704589
-34.344689	-1.985823	1.496435	0.006535	0.704592
-34.564552	-1.951473	1.501440	0.006576	0.704582
-34.505142	-1.958041	1.506445	0.006565	0.704590
-34.844289	-2.038084	1.511450	0.006628	0.704307
-35.667456	-1.917157	1.516454	0.006781	0.704255
-35.194732	-1.995711	1.521459	0.006693	0.704267
-35.095781	-2.019435	1.526464	0.006675	0.704255
-35.460019	-1.950747	1.531469	0.006742	0.704262
-35.614594	-1.922652	1.536474	0.006771	0.704263
-35.424032	-1.960115	1.541478	0.006736	0.704256
-35.542466	-2.069453	1.546483	0.006758	0.703993
-36.649991	-1.895685	1.551488	0.006964	0.703945
-36.545598	-1.910084	1.556493	0.006945	0.703954
-35.978143	-2.012961	1.561498	0.006839	0.703950
-36.526036	-1.915168	1.566502	0.006941	0.703951
-36.218160	-1.965922	1.571507	0.006884	0.703959
-36.220649	-1.969934	1.576512	0.006884	0.703950
-36.401822	-2.061721	1.581517	0.006918	0.703700
-37.092439	-1.969464	1.586522	0.007046	0.703637
-37.284161	-1.937336	1.591526	0.007082	0.703633
-36.878342	-2.006175	1.596531	0.007007	0.703640
-37.500863	-1.898207	1.601536	0.007122	0.703634
-37.218765	-1.945607	1.606541	0.007070	0.703640
-36.900063	-2.002859	1.611546	0.007011	0.703639
-37.868984	-1.967979	1.616550	0.007191	0.703361
-38.167818	-1.920813	1.621555	0.007247	0.703349
-38.088270	-1.938132	1.626560	0.007232	0.703342
-37.783604	-1.988901	1.631565	0.007175	0.703350
-37.963729	-1.957950	1.636570	0.007209	0.703347
-38.014772	-1.953030	1.641574	0.007218	0.703339
-37.636606	-2.017715	1.646579	0.007148	0.703344
-38.693215	-1.998324	1.651584	0.007344	0.703003
-38.875177	-1.962910	1.656589	0.007378	0.703009
-39.041503	-1.934302	1.661594	0.007409	0.703007
-38.997467	-1.943086	1.666598	0.007401	0.703005
-38.706522	-1.991102	1.671603	0.007347	0.703013
-39.217274	-1.907576	1.676608	0.007442	0.702998
-38.847890	-1.969036	1.681613	0.007373	0.703007
-39.216810	-2.027789	1.686618	0.007442	0.702755
-40.097615	-1.903501	1.691622	0.007606	0.702689
-39.744456	-1.962458	1.696627	0.007540	0.702697
-39.798402	-1.957363	1.701632	0.007550	0.702688
-40.071364	-1.906612	1.706637	0.007601	0.702692
-39.557146	-1.997995	1.711642	0.007505	0.702693
-39.729440	-1.969056	1.716646	0.007537	0.702689
-40.236926	-1.990763	1.721651	0.007632	0.702462
-40.923210	-1.915581	1.726656	0.007759	0.702367
-40.445054	-1.997446	1.731661	0.007671	0.702374
-40.473247	-1.992116	1.736666	0.007676	0.702375
-41.008107	-1.899570	1.741670	0.007775	0.702369
-40.442358	-1.995085	1.746675	0.007670	0.702380
-40.496184	-1.990357	1.751680	0.007680	0.702370
-41.047596	-2.009811	1.756685	0.007783	0.702132
-41.482456	-1.958442	1.761690	0.007864	0.702079
-41.458297	-1.967694	1.766694	0.007859	0.702069
-41.506458	-1.954519	1.771699	0.007868	0.702078
-41.825103	-1.901951	1.776704	0.007927	0.702070
-41.302664	-1.990057	1.781709	0.007830	0.702080
-41.257637	-1.999326	1.786714	0.007822	0.702077
-42.369746	-1.963416	1.791718	0.008029	0.701749
-42.411739	-1.955316	1.796723	0.008037	0.701750
-42.646864	-1.916866	1.801728	0.008080	0.701743
-42.436273	-1.952571	1.806733	0.008041	0.701747
-42.286420	-1.978564	1.811738	0.008013	0.701748
-42.558583	-1.933664	1.816742	0.008064	0.701741
-42.422267	-1.952614	1.821747	0.008039	0.701752
-42.571636	-2.035665	1.826752	0.008066	0.701530
-43.213975	-1.966240	1.831757	0.008186	0.701438
-42.965379	-2.011538	1.836762	0.008140	0.701436
-43.358492	-1.944528	1.841766	0.008213	0.701430
-43.180351	-1.970786	1.846771	0.008180	0.701441
-43.285334	-1.956118	1.851776	0.008199	0.701433
-43.424599	-1.930018	1.856781	0.008225	0.701436
-43.890412	-1.994046	1.861786	0.008312	0.701138
-44.020467	-1.981380	1.866790	0.008336	0.701117
-44.048602	-1.971243	1.871795	0.008341	0.701127
-44.169458	-1.953781	1.876800	0.008364	0.701119
-44.092480	-1.965740	1.881805	0.008349	0.701122
-44.043449	-1.973718	1.886810	0.008340	0.701124
-44.457126	-1.903269	1.891814	0.008417	0.701117
-44.301765	-2.043752	1.896819	0.008388	0.700889
-44.705167	-1.980488	1.901824	0.008464	0.700871
-45.015165	-1.921129	1.906829	0.008521	0.700879
-44.782741	-1.964122	1.911834	0.008478	0.700876
-44.896931	-1.948386	1.916838	0.008499	0.700867
-44.788500	-1.962411	1.921843	0.008479	0.700878
-45.124319	-1.979064	1.926848	0.008542	0.700723
-46.036855	-1.909756	1.931853	0.008711	0.700533
-45.451531	-2.013294	1.936858	0.008603	0.700535
-46.006834	-1.917199	1.941862	0.008706	0.700529
-45.776403	-1.952328	1.946867	0.008663	0.700541
-45.769310	-1.958218	1.951872	0.008662	0.700532
-45.825519	-1.947507	1.956877	0.008672	0.700533
-45.925605	-2.012855	1.961882	0.008691	0.700365
-46.782748	-1.934785	1.966886	0.008850	0.700213
-46.267511	-2.019785	1.971891	0.008754	0.700227
-46.697290	-1.946687	1.976896	0.008834	0.700220
-46.693086	-1.946595	1.981901	0.008834	0.700221
-46.363183	-2.005355	1.986906	0.008772	0.700222
-46.664675	-1.954596	1.991910	0.008828	0.700215
-47.099345	-2.016634	1.996915	0.008909	0.699932
-47.529905	-1.958673	2.001920	0.008989	0.699894
-47.586954	-1.948085	2.011917	0.009000	0.699895
-47.545710	-1.954680	2.021914	0.008992	0.699897
-47.447988	-1.972618	2.031910	0.008974	0.699896
-47.544068	-1.956764	2.041907	0.008992	0.699893
-47.581893	-1.950567	2.051904	0.008999	0.699892
-47.577040	-1.951366	2.061901	0.008998	0.699892
-47.680928	-1.932309	2.071898	0.009017	0.699893
-47.508736	-1.962835	2.081894	0.008985	0.699894
-47.597977	-1.948701	2.091891	0.009002	0.699890
-47.589823	-1.950050	2.101888	0.009000	0.699890
-47.663237	-1.936582	2.111885	0.009014	0.699891
-47.609010	-1.946532	2.121882	0.009004	0.699890
-47.093523	-2.038472	2.131878	0.008908	0.699890
-47.166943	-1.895687	2.141875	0.008922	0.700154
-46.554603	-1.976115	2.151872	0.008808	0.700212
-46.782667	-1.934220	2.161869	0.008850	0.700214
-46.495788	-1.984080	2.171866	0.008797	0.700217
-46.641983	-1.953549	2.181862	0.008824	0.700226
-45.882681	-1.939346	2.191859	0.008682	0.700530
-45.700779	-1.972912	2.201856	0.008649	0.700527
-45.774351	-1.957335	2.211853	0.008662	0.700532
-45.638689	-1.980034	2.221850	0.008637	0.700535
-45.113186	-1.948749	2.231846	0.008539	0.700789
-45.075620	-1.916350	2.241843	0.008532	0.700868
-44.697872	-1.983375	2.251840	0.008462	0.700869
-44.784516	-1.967278	2.261837	0.008478	0.700870
-44.144900	-1.984097	2.271834	0.008359	0.701067
-44.244722	-1.939028	2.281830	0.008377	0.701122
-44.030054	-1.978900	2.291827	0.008337	0.701119
-44.180375	-1.919884	2.301824	0.008365	0.701184
-43.282729	-1.957615	2.311821	0.008198	0.701432
-42.987282	-2.010154	2.321818	0.008143	0.701432
-43.370241	-1.941450	2.331814	0.008215	0.701433
-42.860438	-1.923335	2.341811	0.008120	0.701654
-42.367941	-1.969187	2.351808	0.008028	0.701739
-42.433585	-1.957182	2.361805	0.008040	0.701739
-42.080396	-1.983209	2.371802	0.007974	0.701814
-41.702760	-1.922645	2.381798	0.007904	0.702073
-41.573850	-1.946877	2.391795	0.007880	0.702071
-41.525670	-1.957332	2.401792	0.007871	0.702067
-40.954491	-1.938458	2.411789	0.007765	0.702311
-40.602019	-1.972982	2.421786	0.007699	0.702368
-40.711072	-1.953238	2.431782	0.007719	0.702369
-40.480049	-1.941360	2.441779	0.007676	0.702476
-39.591782	-1.995539	2.451776	0.007511	0.702687
-39.856895	-1.947350	2.461773	0.007560	0.702689
-39.896838	-1.939155	2.471770	0.007568	0.702691
-39.166246	-1.936632	2.481766	0.007432	0.702959
-38.843231	-1.971872	2.491763	0.007371	0.703004
-39.071531	-1.933923	2.501760	0.007414	0.702999
-38.820759	-1.912706	2.511757	0.007367	0.703132
-37.981297	-1.959081	2.521754	0.007211	0.703340
-38.133400	-1.932436	2.531750	0.007239	0.703340
-38.023970	-1.953002	2.541747	0.007219	0.703337
-37.479509	-1.904805	2.551744	0.007117	0.703631
-37.182056	-1.958816	2.561741	0.007062	0.703629
-37.070967	-1.978594	2.571738	0.007041	0.703629
-36.946749	-1.923167	2.581734	0.007018	0.703785
-36.089752	-1.995384	2.591731	0.006859	0.703948
-36.608122	-1.903749	2.601728	0.006955	0.703946
-36.089942	-1.991301	2.611725	0.006859	0.703956
-35.533783	-1.942686	2.621722	0.006755	0.704254
-35.509637	-1.947156	2.631718	0.006751	0.704254
-35.254917	-1.992307	2.641715	0.006703	0.704254
-35.287404	-1.897081	2.651712	0.006709	0.704435
-34.415023	-1.978472	2.661709	0.006547	0.704584
-34.462048	-1.969439	2.671706	0.006555	0.704585
-34.524133	-1.957915	2.681702	0.006567	0.704586
-33.899517	-1.925514	2.691699	0.006451	0.704876
-33.884321	-1.925633	2.701696	0.006448	0.704881
-33.651945	-1.967187	2.711693	0.006405	0.704881
-33.302566	-1.931106	2.721690	0.006340	0.705079
-32.606358	-1.990329	2.731686	0.006210	0.705210
-32.503099	-2.009058	2.741683	0.006191	0.705209
-32.833011	-1.951612	2.751680	0.006252	0.705206
-32.026111	-1.952696	2.761677	0.006102	0.705494
-31.948038	-1.951593	2.771674	0.006087	0.705524
-31.837982	-1.972155	2.781670	0.006067	0.705522
-31.649486	-1.929014	2.791667	0.006032	0.705676
-31.046860	-1.946818	2.801664	0.005919	0.705857
-30.868013	-1.977078	2.811661	0.005886	0.705860
-31.062513	-1.943037	2.821658	0.005922	0.705859
-30.225107	-1.982728	2.831654	0.005766	0.706079
-30.388886	-1.930180	2.841651	0.005797	0.706126
-30.294294	-1.948568	2.851648	0.005779	0.706123
-29.851613	-1.958328	2.861645	0.005697	0.706262
-29.336104	-1.960093	2.871642	0.005601	0.706443
-29.160594	-1.990533	2.881638	0.005568	0.706445
-29.681320	-1.882552	2.891635	0.005665	0.706475
-28.460850	-1.964468	2.901632	0.005438	0.706748
-28.550250	-1.946947	2.911629	0.005454	0.706751
-28.660370	-1.926627	2.921626	0.005475	0.706753
-27.809437	-1.959272	2.931622	0.005316	0.706992
-27.661278	-1.939797	2.941619	0.005289	0.707084
-27.577722	-1.956725	2.951616	0.005273	0.707080
-27.483965	-1.941836	2.961613	0.005256	0.707143
-26.952306	-1.919446	2.971610	0.005157	0.707378
-26.727961	-1.959639	2.981606	0.005115	0.707378
-26.781968	-1.950607	2.991603	0.005125	0.707377
-26.116201	-1.933222	3.001600	0.005001	0.707650
-25.894709	-1.948709	3.011597	0.004960	0.707698
-25.945805	-1.940313	3.021594	0.004969	0.707696
-25.641664	-1.934056	3.031590	0.004913	0.707818
-25.018090	-1.948861	3.041587	0.004797	0.708011
-25.081118	-1.938690	3.051584	0.004808	0.708009
-25.041999	-1.946023	3.061581	0.004801	0.708008
-24.191567	-1.934860	3.071578	0.004643	0.708334
-23.874014	-1.982460	3.081574	0.004584	0.708352
-24.075045	-1.949564	3.091571	0.004621	0.708347
-24.023135	-1.925205	3.101568	0.004611	0.708414
-23.457256	-1.915085	3.111565	0.004506	0.708636
-23.183754	-1.964231	3.121562	0.004455	0.708635
-23.274656	-1.947415	3.131558	0.004472	0.708637
-22.679714	-1.908946	3.141555	0.004361	0.708926
-22.391537	-1.947239	3.151552	0.004307	0.708952
-22.292513	-1.965288	3.161549	0.004289	0.708951
-22.311692	-1.895902	3.171546	0.004293	0.709084
-21.238802	-1.999539	3.181542	0.004093	0.709259
-21.579386	-1.939669	3.191539	0.004156	0.709257
-21.461923	-1.960067	3.201536	0.004134	0.709258
-20.936444	-1.897750	3.211533	0.004036	0.709570
-20.362070	-1.988597	3.221530	0.003930	0.709593
-20.621829	-1.943133	3.231526	0.003978	0.709592
-20.424778	-1.914957	3.241523	0.003941	0.709718
-19.621109	-1.972830	3.251520	0.003792	0.709889
-19.847316	-1.933426	3.261517	0.003834	0.709887
-19.773156	-1.946065	3.271514	0.003820	0.709888
-18.967569	-1.939188	3.281510	0.003670	0.710189
-19.067086	-1.908909	3.291507	0.003688	0.710214
-18.760470	-1.963483	3.301504	0.003631	0.710214
-18.761970	-1.891766	3.311501	0.003631	0.710357
-17.597784	-2.011294	3.321498	0.003415	0.710533
-17.917020	-1.954493	3.331494	0.003474	0.710533
-18.029700	-1.933679	3.341491	0.003495	0.710534
-17.044134	-1.969372	3.351488	0.003312	0.710814
-17.088976	-1.934928	3.361485	0.003320	0.710866
-16.801562	-1.983729	3.371482	0.003266	0.710871
-16.884941	-1.960816	3.381478	0.003282	0.710887
-16.342852	-1.931973	3.391475	0.003181	0.711138
-16.457102	-1.912720	3.401472	0.003202	0.711136
-16.259143	-1.948241	3.411469	0.003165	0.711135
-15.727046	-1.920900	3.421466	0.003066	0.711379
-15.473435	-1.929039	3.431462	0.003019	0.711453
-15.492902	-1.925659	3.441459	0.003023	0.711453
-15.093584	-1.926371	3.451456	0.002948	0.711593
-14.609939	-1.930217	3.461453	0.002858	0.711757
-14.425940	-1.962739	3.471450	0.002824	0.711758
-14.669870	-1.910110	3.481446	0.002869	0.711776
-13.498240	-1.963274	3.491443	0.002651	0.712086
-13.477878	-1.966481	3.501440	0.002647	0.712087
-13.420491	-1.976559	3.511437	0.002637	0.712088
-13.508868	-1.918347	3.521434	0.002653	0.712172
-12.765463	-1.944315	3.531430	0.002515	0.712384
-12.604915	-1.971480	3.541427	0.002485	0.712387
-12.739597	-1.950081	3.551424	0.002510	0.712382
-12.197204	-1.907583	3.561421	0.002409	0.712659
-11.767613	-1.958113	3.571418	0.002329	0.712711
-11.803427	-1.951585	3.581414	0.002336	0.712711
-11.743208	-1.903086	3.591411	0.002324	0.712829
-11.143178	-1.913453	3.601408	0.002213	0.713021
-10.880635	-1.960006	3.611405	0.002164	0.713022
-11.015306	-1.935550	3.621402	0.002189	0.713023
-10.207516	-1.911167	3.631398	0.002038	0.713358
-9.696262	-2.000224	3.641395	0.001943	0.713362
-10.196785	-1.912863	3.651392	0.002036	0.713358
-9.903532	-1.926772	3.661389	0.001982	0.713434
-9.070087	-1.966215	3.671386	0.001826	0.713651
-9.038413	-1.971160	3.681382	0.001821	0.713653
-8.749244	-2.022808	3.691379	0.001767	0.713653
-8.720109	-1.938061	3.701376	0.001761	0.713831
-7.633952	-2.063911	3.711373	0.001559	0.713966
-8.049696	-1.989340	3.721370	0.001636	0.713967
-7.737730	-2.044065	3.731366	0.001578	0.713969
-7.368325	-2.034571	3.741363	0.001510	0.714118
-7.031293	-2.017561	3.751360	0.001447	0.714271
-6.949811	-2.032717	3.761357	0.001432	0.714270
-6.828749	-2.053744	3.771354	0.001409	0.714271
-6.643276	-2.009675	3.781350	0.001375	0.714424
-5.858671	-2.059888	3.791347	0.001228	0.714602
-6.247999	-1.990026	3.801344	0.001301	0.714603
-5.775750	-2.072713	3.811341	0.001213	0.714606
-5.713979	-1.985817	3.821338	0.001201	0.714800
-5.122917	-2.037494	3.831334	0.001091	0.714907
-5.149437	-2.033055	3.841331	0.001096	0.714906
-5.315076	-1.988906	3.851328	0.001127	0.714935
-4.387841	-2.007176	3.861325	0.000954	0.715227
-4.397771	-2.004905	3.871322	0.000956	0.715228
-4.029864	-2.069865	3.881318	0.000888	0.715229
-3.883471	-2.013364	3.891315	0.000861	0.715393
-3.194337	-2.061215	3.901312	0.000732	0.715541
-3.170468	-2.065989	3.911309	0.000728	0.715540
-3.572082	-1.994533	3.921306	0.000803	0.715540
-2.690870	-2.031556	3.931302	0.000638	0.715778
-2.601890	-1.995010	3.941299	0.000622	0.715882
-2.411172	-2.030887	3.951296	0.000586	0.715878
-2.326740	-2.036394	3.961293	0.000571	0.715897
-1.732646	-2.025676	3.971290	0.000460	0.716128
-1.661561	-2.037244	3.981286	0.000447	0.716130
-1.896248	-1.997025	3.991283	0.000490	0.716127
-1.454493	-1.960038	4.001280	0.000408	0.716356
-1.416680	-1.922897	4.011277	0.000401	0.716443
-1.248556	-1.951316	4.021274	0.000370	0.716446
-1.111561	-1.845418	4.031270	0.000344	0.716704
-1.042660	-1.831602	4.041267	0.000331	0.716756
-0.751158	-1.841441	4.051264	0.000277	0.716839
-0.737195	-1.724023	4.061261	0.000274	0.717076
-0.605341	-1.745702	4.071258	0.000250	0.717080
-0.610012	-1.604968	4.081254	0.000251	0.717357
-0.731614	-1.571264	4.091251	0.000273	0.717381
-0.723619	-1.425136	4.101248	0.000272	0.717672
-0.907166	-1.351570	4.111245	0.000306	0.717753
-0.581998	-1.279026	4.121242	0.000245	0.718011
-0.504903	-1.201501	4.131238	0.000231	0.718191
-0.332090	-1.151804	4.141235	0.000198	0.718350
-0.346491	-1.012137	4.151232	0.000201	0.718621
-0.344829	-0.931829	4.161229	0.000201	0.718780
-0.328277	-0.833916	4.171226	0.000198	0.718979
-0.166569	-0.717251	4.181222	0.000167	0.719266
-0.150184	-0.600887	4.191219	0.000164	0.719501
-0.097560	-0.494982	4.201216	0.000154	0.719729
-0.233991	-0.349106	4.211213	0.000180	0.719968
-0.067810	-0.238868	4.221210	0.000149	0.720244
0.118552	-0.124627	4.231206	0.000114	0.720534
-0.106009	0.073454	4.241203	0.000155	0.720845
0.000000	0.195669	4.251200	0.000136	0.721123
-0.026951	0.838984	4.256205	0.000140	0.722378
0.007809	2.101078	4.261210	0.000133	0.724864
0.300043	3.896712	4.266214	0.000077	0.728471
0.606629	6.259785	4.271219	0.000019	0.733164
0.747990	9.142737	4.276224	-0.000010	0.738769
1.247221	12.453235	4.281229	-0.000105	0.745267
1.435220	16.275752	4.286234	-0.000142	0.752570
1.747597	20.470541	4.291238	-0.000203	0.760539
2.221768	25.045404	4.296243	-0.000294	0.769180
2.571315	30.000381	4.301248	-0.000363	0.778377
3.174654	35.268446	4.306253	-0.000478	0.788111
3.572402	40.888965	4.311258	-0.000556	0.798288
4.226232	46.761040	4.316262	-0.000682	0.808857
4.843063	52.936767	4.321267	-0.000801	0.819804
5.132352	59.434264	4.326272	-0.000859	0.831056
5.529001	66.139825	4.331277	-0.000937	0.842541
6.161881	73.021989	4.336282	-0.001059	0.854233
8.484083	79.818807	4.341286	-0.001496	0.866115
13.243185	86.457354	4.346291	-0.002387	0.878271
13.470941	94.074724	4.351296	-0.002434	0.890549
14.102958	101.784518	4.356301	-0.002557	0.902916
14.813353	109.620873	4.361306	-0.002694	0.915334
15.881061	117.498242	4.366310	-0.002898	0.927743
16.881293	125.533705	4.371315	-0.003089	0.940208
17.569012	133.707982	4.376320	-0.003223	0.952635
19.084463	141.841694	4.381325	-0.003510	0.965054
19.896092	150.184246	4.386330	-0.003667	0.977439
21.275793	158.491714	4.391334	-0.003929	0.989761
22.433425	166.899250	4.396339	-0.004150	1.002017
23.065436	175.429515	4.401344	-0.004274	1.014168
23.975966	183.952812	4.406349	-0.004449	1.026232
24.328202	192.609229	4.411354	-0.004520	1.038205
24.957763	201.224732	4.416358	-0.004643	1.050050
25.908835	209.819242	4.421363	-0.004825	1.061810
26.959731	218.418760	4.426368	-0.005027	1.073469
28.058264	227.011964	4.431373	-0.005237	1.085005
28.694272	235.705494	4.436378	-0.005361	1.096446
29.299909	244.389637	4.441382	-0.005479	1.107750
30.879748	252.934227	4.446387	-0.005779	1.118974
31.855711	261.568296	4.451392	-0.005966	1.130068
33.075153	270.182979	4.456397	-0.006199	1.141082
33.856771	278.886732	4.461402	-0.006350	1.152007
34.570180	287.547043	4.466406	-0.006489	1.162761
35.561764	296.161248	4.471411	-0.006679	1.173419
36.313240	304.785812	4.476416	-0.006825	1.183943
37.251246	313.399720	4.481421	-0.007005	1.194400
37.907515	322.018434	4.486426	-0.007133	1.204714
38.322529	330.687930	4.491430	-0.007216	1.214952
39.045001	339.266234	4.496435	-0.007356	1.225059
39.933772	347.824459	4.501440	-0.007527	1.235092
41.093420	356.298795	4.506445	-0.007748	1.245001
41.604344	364.889311	4.511450	-0.007849	1.254838
42.361943	373.409440	4.516454	-0.007996	1.264566
43.109367	381.939655	4.521459	-0.008140	1.274229
43.400302	390.498866	4.526464	-0.008200	1.283766
44.026880	399.006647	4.531469	-0.008322	1.293238
45.049757	407.430329	4.536474	-0.008518	1.302622
45.561563	416.011058	4.541478	-0.008619	1.312015
46.253232	424.491439	4.546483	-0.008754	1.321266
47.122471	432.869470	4.551488	-0.008921	1.330375
48.236260	441.214324	4.556493	-0.009134	1.339430
49.443276	449.536500	4.561498	-0.009364	1.348416
50.039622	457.972967	4.566502	-0.009480	1.357355
50.707587	466.372115	4.571507	-0.009610	1.366209
51.059770	474.828680	4.576512	-0.009681	1.375010
51.625035	483.218061	4.581517	-0.009792	1.383723
52.419423	491.581809	4.586522	-0.009945	1.392394
52.771600	499.975491	4.591526	-0.010017	1.400967
53.483826	508.309396	4.596531	-0.010155	1.409487
53.758742	516.705619	4.601536	-0.010211	1.417946
54.355036	525.026612	4.606541	-0.010328	1.426333
54.898210	533.368333	4.611546	-0.010434	1.434682
55.358817	541.699637	4.616550	-0.010525	1.442959
56.008397	550.003623	4.621555	-0.010652	1.451192
56.711178	558.289097	4.626560	-0.010788	1.459369
57.448903	566.575905	4.631565	-0.010931	1.467507
57.897750	574.956013	4.636570	-0.011020	1.475644
58.483086	583.214687	4.641574	-0.011134	1.483642
58.975076	591.515954	4.646579	-0.011231	1.491623
59.490545	599.788487	4.651584	-0.011333	1.499537
59.887167	608.075345	4.656589	-0.011412	1.507405
60.591056	616.313921	4.661594	-0.011548	1.515233
61.059080	624.569490	4.666598	-0.011641	1.523001
61.540321	632.847495	4.671603	-0.011736	1.530752
61.670119	641.158890	4.676608	-0.011766	1.538442
62.500532	649.344295	4.681613	-0.011925	1.546083
62.943429	657.628037	4.686618	-0.012013	1.553718
63.524086	665.838603	4.691622	-0.012127	1.561269
64.028982	674.079094	4.696627	-0.012226	1.568800
64.675056	682.280593	4.701632	-0.012352	1.576280
65.244222	690.506161	4.706637	-0.012463	1.583735
65.684766	698.751050	4.711642	-0.012551	1.591153
66.031886	707.001727	4.716646	-0.012621	1.598529
66.882125	715.153011	4.721651	-0.012784	1.605854
66.966968	723.444476	4.726656	-0.012805	1.613161
67.358600	731.666858	4.731661	-0.012884	1.620418
67.801938	739.882259	4.736666	-0.012972	1.627643
68.225829	748.148996	4.741670	-0.013056	1.634878
68.838023	756.307887	4.746675	-0.013175	1.642014
69.214212	764.500063	4.751680	-0.013251	1.649115
69.529711	772.727994	4.756685	-0.013315	1.656208
70.161673	780.877473	4.761690	-0.013438	1.663246
70.641253	789.069638	4.766694	-0.013532	1.670270
71.450340	797.225002	4.771699	-0.013688	1.677278
71.758110	805.408432	4.776704	-0.013751	1.684213
72.140388	813.608399	4.781709	-0.013828	1.691143
72.686449	821.781195	4.786714	-0.013935	1.698044
73.248931	829.927556	4.791718	-0.014045	1.704897
73.701629	838.141038	4.796723	-0.014134	1.711763
74.013120	846.331599	4.801728	-0.014198	1.718565
74.232377	854.509736	4.806733	-0.014244	1.725317
74.644380	862.697750	4.811738	-0.014326	1.732076
75.111829	870.847207	4.816742	-0.014418	1.738784
75.745682	878.976417	4.821747	-0.014542	1.745471
76.066457	887.167887	4.826752	-0.014607	1.752144
76.823809	895.287849	4.831757	-0.014753	1.758787
77.403393	903.411359	4.836762	-0.014866	1.765387
77.655752	911.617435	4.841766	-0.014918	1.771986
78.243728	919.774129	4.846771	-0.015033	1.778564
78.648246	927.912975	4.851776	-0.015114	1.785080
79.211267	936.096308	4.856781	-0.015224	1.791627
79.604437	944.273823	4.861786	-0.015303	1.798125
80.071171	952.380595	4.866790	-0.015395	1.804552
80.375534	960.568009	4.871795	-0.015457	1.811000
80.689467	968.713706	4.876800	-0.015521	1.817394
81.088678	976.849524	4.881805	-0.015600	1.823768
81.631313	984.977592	4.886810	-0.015707	1.830130
82.109677	993.111156	4.891814	-0.015801	1.836467
82.714271	1001.227888	4.896819	-0.015919	1.842784
83.241104	1009.351548	4.901824	-0.016022	1.849075
83.415894	1017.556711	4.906829	-0.016060	1.855366
83.805258	1025.689536	4.911834	-0.016138	1.861606
84.302649	1033.802420	4.916838	-0.016236	1.867822
84.637139	1041.997431	4.921843	-0.016303	1.874060
84.740101	1050.132817	4.926848	-0.016328	1.880206
85.282997	1058.214246	4.931853	-0.016434	1.886342
86.038778	1066.305793	4.936858	-0.016580	1.892490
86.290869	1074.448262	4.941862	-0.016633	1.898598
86.822192	1082.555961	4.946867	-0.016737	1.904692
87.158585	1090.699618	4.951872	-0.016805	1.910772
87.681719	1098.826496	4.956877	-0.016907	1.916840
87.952162	1106.955846	4.961882	-0.016963	1.922863
88.278442	1115.082739	4.966886	-0.017029	1.928872
88.852367	1123.196697	4.971891	-0.017141	1.934879
89.171378	1131.317583	4.976896	-0.017206	1.940845
89.678802	1139.425141	4.981901	-0.017306	1.946803
90.476573	1147.537266	4.986906	-0.017460	1.952778
90.997205	1155.641716	4.991910	-0.017562	1.958699
91.223973	1163.771789	4.996915	-0.017609	1.964589
91.536532	1171.885179	5.001920	-0.017673	1.970458
92.232662	1179.961220	5.006925	-0.017808	1.976324
92.473460	1188.094527	5.011930	-0.017858	1.982165
92.674935	1196.227859	5.016934	-0.017901	1.987984
93.128786	1204.351654	5.021939	-0.017990	1.993806
93.386550	1212.461869	5.026944	-0.018044	1.999581
93.719787	1220.554711	5.031949	-0.018111	2.005335
94.495738	1228.628390	5.036954	-0.018261	2.011105
95.005296	1236.726815	5.041958	-0.018361	2.016848
95.686326	1244.810944	5.046963	-0.018493	2.022582
95.852560	1252.956695	5.051968	-0.018529	2.028290
96.483773	1261.078608	5.056973	-0.018652	2.034013
96.887996	1269.170903	5.061978	-0.018733	2.039676
97.028414	1277.271077	5.066982	-0.018764	2.045301
97.597693	1285.363360	5.071987	-0.018875	2.050949
97.777446	1293.497595	5.076992	-0.018914	2.056572
98.219883	1301.568500	5.081997	-0.019002	2.062161
98.634042	1309.658732	5.087002	-0.019084	2.067746
98.835972	1317.804205	5.092006	-0.019127	2.073332
99.201552	1325.894998	5.097011	-0.019201	2.078882
99.565511	1333.962188	5.102016	-0.019274	2.084401
100.134007	1342.031025	5.107021	-0.019385	2.089927
100.585724	1350.148797	5.112026	-0.019474	2.095460
101.154818	1358.202304	5.117030	-0.019585	2.100946
101.863919	1366.269841	5.122035	-0.019723	2.106440
102.223551	1374.430019	5.127040	-0.019795	2.111948
102.624924	1382.554375	5.132045	-0.019875	2.117422
103.207246	1390.589909	5.137050	-0.019989	2.122840
103.441331	1398.689508	5.142054	-0.020037	2.128254
103.907432	1406.791879	5.147059	-0.020130	2.133677
104.189157	1414.875138	5.152064	-0.020187	2.139056
104.742389	1422.936036	5.157069	-0.020296	2.144433
105.103643	1431.044366	5.162074	-0.020368	2.149809
105.134691	1439.183144	5.167078	-0.020379	2.155161
105.763206	1447.224483	5.172083	-0.020501	2.160491
106.172622	1455.300430	5.177088	-0.020583	2.165811
106.368574	1463.417356	5.182093	-0.020625	2.171124
106.847874	1471.492911	5.187098	-0.020719	2.176424
107.283913	1479.552288	5.192102	-0.020806	2.181696
107.813872	1487.637972	5.197107	-0.020910	2.186980
107.682645	1495.807463	5.202112	-0.020891	2.192246
108.339579	1503.850658	5.207117	-0.021018	2.197489
108.981651	1511.888432	5.212122	-0.021143	2.202715
109.229218	1519.962892	5.217126	-0.021194	2.207916
109.498886	1528.096462	5.222131	-0.021250	2.213145
109.882644	1536.152649	5.227136	-0.021327	2.218322
110.181838	1544.230003	5.232141	-0.021387	2.223493
110.466217	1552.329697	5.237146	-0.021446	2.228665
110.958655	1560.394397	5.242150	-0.021543	2.233821
111.479912	1568.447381	5.247155	-0.021645	2.238960
111.721014	1576.523937	5.252160	-0.021695	2.244078
112.088169	1584.598811	5.257165	-0.021769	2.249193
112.713170	1592.684317	5.262170	-0.021890	2.254327
113.005905	1600.744874	5.267174	-0.021950	2.259403
113.295354	1608.842733	5.272179	-0.022009	2.264492
113.625391	1616.932856	5.277184	-0.022076	2.269567
114.016941	1625.090566	5.282189	-0.022154	2.274679
114.718229	1633.088727	5.287194	-0.022290	2.279706
114.983884	1641.148783	5.292198	-0.022345	2.284724
115.402851	1649.220283	5.297203	-0.022428	2.289750
115.544945	1657.327920	5.302208	-0.022460	2.294764
115.994382	1665.361659	5.307213	-0.022549	2.299748
116.728334	1673.383769	5.312218	-0.022691	2.304738
116.823581	1681.496526	5.317222	-0.022714	2.309718
117.143379	1689.604065	5.322227	-0.022779	2.314703
117.439254	1697.645525	5.327232	-0.022839	2.319636
117.800406	1705.696947	5.332237	-0.022911	2.324569
117.942720	1713.805322	5.337242	-0.022943	2.329508
118.108586	1721.895342	5.342246	-0.022979	2.334428
118.565208	1729.953233	5.347251	-0.023070	2.339341
118.811921	1738.013652	5.352256	-0.023121	2.344229
119.208340	1746.082717	5.357261	-0.023200	2.349123
119.705139	1754.188835	5.362266	-0.023298	2.354038
119.995500	1762.218518	5.367270	-0.023357	2.358880
120.192486	1770.305683	5.372275	-0.023399	2.363739
120.600928	1778.345326	5.377280	-0.023480	2.368576
120.805312	1786.448524	5.382285	-0.023524	2.373425
121.220381	1794.499712	5.387290	-0.023606	2.378250
121.729217	1802.527340	5.392294	-0.023706	2.383059
122.287012	1810.579474	5.397299	-0.023815	2.387876
122.553586	1818.664999	5.402304	-0.023870	2.392680
123.053640	1826.713291	5.407309	-0.023968	2.397470
123.689394	1834.733409	5.412314	-0.024092	2.402246
123.797715	1842.823652	5.417318	-0.024118	2.407011
123.954640	1850.945383	5.422323	-0.024152	2.411789
124.176274	1859.015249	5.427328	-0.024199	2.416533
124.556399	1867.053923	5.432333	-0.024275	2.421261
124.856071	1875.114395	5.437338	-0.024336	2.425986
125.012867	1883.217182	5.442342	-0.024370	2.430716
125.554490	1891.334834	5.447347	-0.024476	2.435474
125.868613	1899.345936	5.452352	-0.024540	2.440144
126.160215	1907.373130	5.457357	-0.024600	2.444813
126.663022	1915.420578	5.462362	-0.024698	2.449500
126.669924	1923.515760	5.467366	-0.024705	2.454169
126.891553	1931.587117	5.472371	-0.024752	2.458831
127.195881	1939.619609	5.477376	-0.024813	2.463468
127.527221	1947.666910	5.482381	-0.024880	2.468106
127.705679	1955.770802	5.487386	-0.024919	2.472757
127.962356	1963.809864	5.492390	-0.024972	2.477368
128.461238	1971.833413	5.497395	-0.025070	2.481979
128.828983	1979.868912	5.502400	-0.025144	2.486579
129.162205	1987.935836	5.507405	-0.025211	2.491186
129.607583	1996.002848	5.512410	-0.025299	2.495792
129.759206	2004.060335	5.517414	-0.025333	2.500363
130.134024	2012.110790	5.522419	-0.025408	2.504937
130.565905	2020.167749	5.527424	-0.025493	2.509511
130.952698	2028.266032	5.532429	-0.025571	2.514097
131.226999	2036.337340	5.537434	-0.025627	2.518651
131.194490	2044.386432	5.542438	-0.025626	2.523162
131.688370	2052.417136	5.547443	-0.025724	2.527692
132.051127	2060.462829	5.552448	-0.025796	2.532214
132.315160	2068.537137	5.557453	-0.025851	2.536736
132.746011	2076.577826	5.562458	-0.025936	2.541243
132.965851	2084.610155	5.567462	-0.025982	2.545722
133.564608	2092.676789	5.572467	-0.026099	2.550240
133.550283	2100.781145	5.577472	-0.026102	2.554726
133.930549	2108.798331	5.582477	-0.026178	2.559185
134.420125	2116.834886	5.587482	-0.026274	2.563654
134.689424	2124.879269	5.592486	-0.026330	2.568104
135.028958	2132.954495	5.597491	-0.026398	2.572568
135.358865	2141.018138	5.602496	-0.026465	2.577018
135.548366	2149.080503	5.607501	-0.026505	2.581449
136.181068	2157.085807	5.612506	-0.026628	2.585872
136.651678	2165.148119	5.617510	-0.026721	2.590307
136.786484	2173.444521	5.622515	-0.026752	2.594839
137.050112	2181.402397	5.627520	-0.026806	2.599188
137.269617	2189.403136	5.632525	-0.026852	2.603549
137.484329	2197.433295	5.637530	-0.026897	2.607919
137.530172	2205.503247	5.642534	-0.026911	2.612292
138.009504	2213.524861	5.647539	-0.027006	2.616661
138.369576	2221.540795	5.652544	-0.027078	2.621011
138.486297	2229.592260	5.657549	-0.027105	2.625356
138.554359	2237.665187	5.662554	-0.027123	2.629703
138.933741	2245.702650	5.667558	-0.027199	2.634044
139.499958	2253.717486	5.672563	-0.027309	2.638378
139.962379	2261.735256	5.677568	-0.027401	2.642700
140.227559	2269.785088	5.682573	-0.027455	2.647019
140.615807	2277.860680	5.687578	-0.027533	2.651352
140.709374	2285.937083	5.692582	-0.027556	2.655659
140.880124	2293.993729	5.697587	-0.027593	2.659954
141.290427	2302.010745	5.702592	-0.027674	2.664237
141.420444	2310.080936	5.707597	-0.027704	2.668522
141.894897	2318.138253	5.712602	-0.027797	2.672816
142.347562	2326.166510	5.717606	-0.027887	2.677087
142.774735	2334.191399	5.722611	-0.027972	2.681347
142.960743	2342.237720	5.727616	-0.028011	2.685596
143.268021	2350.276904	5.732621	-0.028074	2.689842
143.590549	2358.368209	5.737626	-0.028139	2.694110
143.740907	2366.401462	5.742630	-0.028173	2.698329
144.128686	2374.427802	5.747635	-0.028250	2.702554
144.557607	2382.469770	5.752640	-0.028335	2.706782
145.023870	2390.535071	5.757645	-0.028427	2.711018
145.130303	2398.640710	5.762650	-0.028452	2.715247
145.554601	2406.614743	5.767654	-0.028536	2.719419
145.507917	2414.705571	5.772659	-0.028533	2.723617
145.817686	2422.736901	5.777664	-0.028596	2.727800
146.409119	2430.747875	5.782669	-0.028711	2.731983
146.799133	2438.828018	5.787674	-0.028789	2.736182
146.850029	2446.857433	5.792678	-0.028804	2.740329
147.199542	2454.888598	5.797683	-0.028874	2.744488
147.612197	2462.933202	5.802688	-0.028956	2.748651
147.767116	2471.063203	5.807693	-0.028990	2.752837
148.148823	2479.110150	5.812698	-0.029067	2.756987
148.619009	2487.084011	5.817702	-0.029160	2.761099
149.085862	2495.115637	5.822707	-0.029252	2.765233
149.201123	2503.157885	5.827712	-0.029278	2.769346
149.491911	2511.226578	5.832717	-0.029338	2.773477
149.843184	2519.259906	5.837722	-0.029408	2.777587
150.017886	2527.287797	5.842726	-0.029446	2.781678
150.547394	2535.307896	5.847731	-0.029550	2.785779
150.907931	2543.362821	5.852736	-0.029622	2.789883
151.275824	2551.434519	5.857741	-0.029696	2.793989
151.442864	2559.495790	5.862746	-0.029733	2.798072
151.594503	2567.503839	5.867750	-0.029766	2.802121
152.174776	2575.521885	5.872755	-0.029879	2.806194
152.271858	2583.611885	5.877760	-0.029903	2.810270
152.616068	2591.668498	5.882765	-0.029972	2.814337
153.128829	2599.697697	5.887770	-0.030073	2.818394
153.398818	2607.706060	5.892774	-0.030128	2.822421
153.514952	2615.775464	5.897779	-0.030155	2.826463
153.767470	2623.827791	5.902784	-0.030207	2.830499
153.988507	2631.918525	5.907789	-0.030254	2.834547
154.215477	2639.945626	5.912794	-0.030301	2.838558
154.160619	2647.965331	5.917798	-0.030296	2.842543
154.603751	2655.996433	5.922803	-0.030384	2.846556
154.720762	2664.047678	5.927808	-0.030411	2.850555
155.071958	2672.076905	5.932813	-0.030482	2.854551
155.352431	2680.124928	5.937818	-0.030539	2.858547
155.578224	2688.125366	5.942822	-0.030587	2.862510
155.963771	2696.175452	5.947827	-0.030664	2.866501
156.552954	2704.193196	5.952832	-0.030778	2.870482
157.132128	2712.222251	5.957837	-0.030892	2.874462
157.285625	2720.290626	5.962842	-0.030925	2.878433
157.411613	2728.329345	5.967846	-0.030954	2.882382
157.603262	2736.380781	5.972851	-0.030995	2.886335
157.881331	2744.434395	5.977856	-0.031052	2.890289
158.045023	2752.486945	5.982861	-0.031088	2.894231
158.688661	2760.503786	5.987866	-0.031213	2.898175
158.822026	2768.538322	5.992870	-0.031243	2.902096
159.110113	2776.600116	5.997875	-0.031302	2.906032
159.496071	2784.619122	6.002880	-0.031379	2.909948
159.619858	2792.770096	6.007885	-0.031407	2.913908
159.952064	2800.775837	6.012890	-0.031474	2.917804
160.127694	2808.777985	6.017894	-0.031512	2.921684
160.308625	2816.807752	6.022899	-0.031551	2.925573
160.493116	2824.812305	6.027904	-0.031591	2.929444
160.714490	2832.885128	6.032909	-0.031637	2.933346
160.988750	2840.915670	6.037914	-0.031694	2.937224
161.191303	2848.935518	6.042918	-0.031737	2.941089
161.460516	2856.952288	6.047923	-0.031792	2.944950
161.865646	2864.976094	6.052928	-0.031873	2.948816
162.077630	2873.052419	6.057933	-0.031917	2.952693
162.454383	2881.115165	6.062938	-0.031993	2.956566
162.509397	2889.139577	6.067942	-0.032008	2.960400
162.771581	2897.154777	6.072947	-0.032062	2.964235
162.885229	2905.201034	6.077952	-0.032089	2.968072
163.000735	2913.251659	6.082957	-0.032115	2.971906
163.385168	2921.316887	6.087962	-0.032192	2.975756
163.627828	2929.281435	6.092966	-0.032243	2.979545
164.119621	2937.324689	6.097971	-0.032339	2.983380
164.367874	2945.382662	6.102976	-0.032391	2.987205
164.568285	2953.415844	6.107981	-0.032434	2.991010
164.904503	2961.480071	6.112986	-0.032501	2.994832
165.027519	2969.499768	6.117990	-0.032530	2.998617
165.223231	2977.539255	6.122995	-0.032571	3.002411
165.643438	2985.544766	6.128000	-0.032655	3.006195
165.962338	2993.553276	6.133005	-0.032719	3.009970
166.417758	3001.610322	6.138010	-0.032809	3.013770
166.547290	3009.643212	6.143014	-0.032839	3.017538
166.563067	3017.721491	6.148019	-0.032847	3.021317
166.748613	3025.731319	6.153024	-0.032887	3.025068
167.155585	3033.756916	6.158029	-0.032968	3.028831
167.521239	3041.824501	6.163034	-0.033041	3.032608
167.468183	3049.898137	6.168038	-0.033036	3.036363
167.811903	3057.903673	6.173043	-0.033106	3.040100
168.058144	3065.911828	6.178048	-0.033157	3.043829
168.107075	3073.956367	6.183053	-0.033171	3.047561
168.413425	3082.028806	6.188058	-0.033233	3.051314
168.763335	3090.047431	6.193062	-0.033304	3.055039
168.858996	3098.083186	6.198067	-0.033327	3.058756
169.355443	3106.087718	6.203072	-0.033424	3.062472
169.474299	3114.120501	6.208077	-0.033452	3.066179
169.951915	3122.161083	6.213082	-0.033546	3.069902
169.960964	3130.294059	6.218086	-0.033553	3.073641
170.400323	3138.306797	6.223091	-0.033640	3.077340
170.663700	3146.321375	6.228096	-0.033694	3.081028
170.934991	3154.279417	6.233101	-0.033750	3.084685
171.296869	3162.314376	6.238106	-0.033823	3.088377
171.597278	3170.336628	6.243110	-0.033884	3.092057
172.109703	3178.379425	6.248115	-0.033984	3.095751
172.294521	3186.410186	6.253120	-0.034024	3.099420
172.402877	3194.437647	6.258125	-0.034050	3.103079
172.613642	3202.495310	6.263130	-0.034094	3.106753
172.737404	3210.537615	6.268134	-0.034122	3.110411
173.332230	3218.552136	6.273139	-0.034238	3.114074
173.738972	3226.564783	6.278144	-0.034319	3.117723
173.745949	3234.638461	6.283149	-0.034326	3.121377
173.998329	3242.644081	6.288154	-0.034378	3.125008
174.406400	3250.670035	6.293158	-0.034459	3.128650
174.894108	3258.716395	6.298163	-0.034555	3.132300
175.176025	3266.763545	6.303168	-0.034613	3.135938
175.444387	3274.761119	6.308173	-0.034668	3.139548
175.731463	3282.794007	6.313178	-0.034727	3.143171
175.762368	3290.850268	6.318182	-0.034738	3.146789
176.206309	3298.874757	6.323187	-0.034826	3.150406
176.444976	3306.951042	6.328192	-0.034876	3.154033
176.563493	3314.975826	6.333197	-0.034903	3.157628
176.758826	3323.011446	6.338202	-0.034944	3.161228
176.922174	3331.004839	6.343206	-0.034980	3.164802
177.121606	3339.044505	6.348211	-0.035022	3.168395
177.358286	3347.104538	6.353216	-0.035072	3.171994
177.663397	3355.123013	6.358221	-0.035134	3.175574
177.808521	3363.166081	6.363226	-0.035166	3.179154
177.851659	3371.192890	6.368230	-0.035179	3.182718
178.215854	3379.216997	6.373235	-0.035252	3.186290
178.547941	3387.249134	6.378240	-0.035320	3.189861
178.797138	3395.280694	6.383245	-0.035371	3.193424
179.216704	3403.338367	6.388250	-0.035455	3.197001
179.458033	3411.327363	6.393254	-0.035505	3.200537
179.675180	3419.343202	6.398259	-0.035550	3.204079
179.663191	3427.420213	6.403264	-0.035553	3.207635
179.760941	3435.435458	6.408269	-0.035577	3.211165
180.168228	3443.464537	6.413274	-0.035658	3.214709
180.084903	3451.514654	6.418278	-0.035648	3.218239
180.400470	3459.521178	6.423283	-0.035712	3.221762
180.714865	3467.533171	6.428288	-0.035775	3.225283
180.841727	3475.591603	6.433293	-0.035804	3.228813
181.108645	3483.698766	6.438298	-0.035859	3.232366
181.253038	3491.726192	6.443302	-0.035891	3.235876
181.378629	3499.691076	6.448307	-0.035920	3.239353
181.733338	3507.697147	6.453312	-0.035991	3.242854
182.126602	3515.705614	6.458317	-0.036070	3.246354
182.615061	3523.713419	6.463322	-0.036166	3.249853
182.680918	3531.779812	6.468326	-0.036183	3.253357
182.429473	3539.865367	6.473331	-0.036142	3.256854
183.085849	3547.835867	6.478336	-0.036269	3.260332
183.198624	3555.858449	6.483341	-0.036295	3.263808
183.354573	3563.922560	6.488346	-0.036330	3.267299
183.550514	3571.930242	6.493350	-0.036371	3.270765
183.950841	3579.979357	6.498355	-0.036451	3.274252
184.037016	3588.019354	6.503360	-0.036473	3.277719
184.496474	3596.004365	6.508365	-0.036563	3.281174
184.931747	3604.005291	6.513370	-0.036650	3.284630
185.048974	3612.076988	6.518374	-0.036677	3.288101
185.291072	3620.119835	6.523379	-0.036727	3.291561
185.796522	3628.134515	6.528384	-0.036826	3.295015
185.945025	3636.143854	6.533389	-0.036859	3.298450
186.016600	3644.215970	6.538394	-0.036878	3.301905
186.265244	3652.225956	6.543398	-0.036929	3.305336
186.716220	3660.250546	6.548403	-0.037019	3.308778
186.725426	3668.330992	6.553408	-0.037026	3.312223
186.823054	3676.343817	6.558413	-0.037049	3.315639
187.318113	3684.348191	6.563418	-0.037146	3.319063
187.493828	3692.356162	6.568422	-0.037184	3.322473
187.915983	3700.358860	6.573427	-0.037268	3.325886
188.463075	3708.381116	6.578432	-0.037375	3.329309
188.519954	3716.430508	6.583437	-0.037391	3.332721
188.680116	3724.514584	6.588442	-0.037426	3.336148
188.778071	3732.493535	6.593446	-0.037450	3.339525
189.362675	3740.505570	6.598451	-0.037564	3.342931
189.366955	3748.594212	6.603456	-0.037570	3.346344
189.573477	3756.583933	6.608461	-0.037613	3.349719
189.916362	3764.652374	6.613466	-0.037683	3.353129
190.073482	3772.703634	6.618470	-0.037717	3.356521
190.225204	3780.687766	6.623475	-0.037750	3.359882
190.409096	3788.709948	6.628480	-0.037790	3.363256
190.540670	3796.758168	6.633485	-0.037820	3.366636
190.744566	3804.794946	6.638490	-0.037863	3.370010
191.006770	3812.808043	6.643494	-0.037917	3.373373
191.308249	3820.834892	6.648499	-0.037978	3.376740
191.422562	3828.855874	6.653504	-0.038005	3.380094
191.578232	3836.879885	6.658509	-0.038039	3.383448
191.863030	3844.923509	6.663514	-0.038097	3.386811
192.041288	3852.934744	6.668518	-0.038136	3.390153
192.481048	3861.061130	6.673523	-0.038223	3.393549
192.681614	3869.083662	6.678528	-0.038266	3.396891
192.831316	3877.038706	6.683533	-0.038299	3.400199
193.398133	3885.035271	6.688538	-0.038409	3.403535
193.390066	3893.065990	6.693542	-0.038413	3.406863
193.799553	3901.076649	6.698547	-0.038495	3.410193
193.981199	3909.145198	6.703552	-0.038534	3.413536
194.231339	3917.135944	6.708557	-0.038585	3.416846
194.431766	3925.171963	6.713562	-0.038628	3.420170
194.675169	3933.193425	6.718566	-0.038679	3.423485
194.730728	3941.242005	6.723571	-0.038694	3.426803
194.982206	3949.258076	6.728576	-0.038746	3.430110
195.688627	3957.245579	6.733581	-0.038883	3.433418
196.092167	3965.316014	6.738586	-0.038963	3.436746
196.117004	3973.301964	6.743590	-0.038973	3.440024
196.410846	3981.321718	6.748595	-0.039033	3.443322
196.808682	3989.375205	6.753600	-0.039112	3.446633
196.707359	3997.395263	6.758605	-0.039099	3.449911
197.220445	4005.458985	6.763610	-0.039200	3.453224
197.502480	4013.491141	6.768614	-0.039257	3.456514
197.602244	4021.503594	6.773619	-0.039281	3.459786
197.934309	4029.504337	6.778624	-0.039348	3.463058
198.060730	4037.539189	6.783629	-0.039377	3.466334
198.407962	4045.581791	6.788634	-0.039447	3.469617
198.558984	4053.653907	6.793638	-0.039480	3.472902
198.851300	4061.690245	6.798643	-0.039540	3.476175
199.236119	4069.671551	6.803648	-0.039617	3.479425
199.402011	4077.645391	6.808653	-0.039653	3.482662
199.456934	4085.733428	6.813658	-0.039668	3.485938
199.537514	4093.725170	6.818662	-0.039689	3.489174
199.730594	4101.768129	6.823667	-0.039730	3.492430
199.733959	4109.833496	6.828672	-0.039736	3.495687
199.981103	4117.800692	6.833677	-0.039787	3.498908
200.321408	4125.823920	6.838682	-0.039856	3.502152
200.536348	4133.826450	6.843686	-0.039901	3.505381
200.786855	4141.865552	6.848691	-0.039953	3.508623
201.159119	4149.908268	6.853696	-0.040027	3.511867
201.320333	4157.957708	6.858701	-0.040063	3.515103
201.716683	4165.926542	6.863706	-0.040142	3.518312
201.806414	4173.972272	6.868710	-0.040163	3.521539
201.869179	4181.983024	6.873715	-0.040180	3.524749
202.124273	4190.055188	6.878720	-0.040233	3.527986
202.405201	4198.055560	6.883725	-0.040291	3.531192
202.842180	4206.092983	6.888730	-0.040377	3.534414
202.721292	4214.164412	6.893734	-0.040360	3.537631
202.740977	4222.181614	6.898739	-0.040369	3.540827
203.116925	4230.178529	6.903744	-0.040444	3.544022
203.128545	4238.213278	6.908749	-0.040452	3.547219
203.430554	4246.261091	6.913754	-0.040513	3.550427
203.747128	4254.346703	6.918758	-0.040577	3.553647
204.056011	4262.357714	6.923763	-0.040640	3.556835
204.380636	4270.306342	6.928768	-0.040706	3.559995
204.440759	4278.300673	6.933773	-0.040722	3.563163
204.827827	4286.376710	6.938778	-0.040799	3.566370
204.863281	4294.342271	6.943782	-0.040811	3.569520
204.880420	4302.420616	6.948787	-0.040820	3.572712
205.158715	4310.480759	6.953792	-0.040877	3.575900
205.264573	4318.432480	6.958797	-0.040902	3.579039
205.448227	4326.466447	6.963802	-0.040941	3.582209
205.732473	4334.469370	6.968806	-0.040999	3.585367
205.890470	4342.502126	6.973811	-0.041034	3.588530
206.063451	4350.561637	6.978816	-0.041071	3.591701
206.305748	4358.554936	6.983821	-0.041122	3.594846
206.324965	4366.604817	6.988826	-0.041130	3.598003
206.585817	4374.599844	6.993830	-0.041184	3.601143
206.490650	4382.597881	6.998835	-0.041172	3.604272
206.854740	4390.648374	7.003840	-0.041245	3.607431
207.036688	4398.623130	7.008845	-0.041284	3.610553
207.247221	4406.706038	7.013850	-0.041328	3.613715
207.688553	4414.734992	7.018854	-0.041416	3.616859
207.976789	4422.717017	7.023859	-0.041475	3.619978
208.098067	4430.757892	7.028864	-0.041502	3.623113
208.111792	4438.778811	7.033869	-0.041510	3.626235
208.556937	4446.811063	7.038874	-0.041598	3.629369
208.805483	4454.875419	7.043878	-0.041650	3.632509
209.041046	4462.902705	7.048883	-0.041699	3.635630
209.069679	4470.923144	7.053888	-0.041710	3.638741
209.326418	4478.925842	7.058893	-0.041763	3.641848
209.520954	4486.949464	7.063898	-0.041804	3.644959
209.450080	4494.971616	7.068902	-0.041796	3.648060
209.751884	4502.980701	7.073907	-0.041858	3.651163
210.003047	4511.049545	7.078912	-0.041910	3.654285
210.336250	4519.062339	7.083917	-0.041977	3.657385
210.488771	4527.065184	7.088922	-0.042010	3.660474
210.603090	4535.099347	7.093926	-0.042037	3.663571
210.849679	4543.105462	7.098931	-0.042088	3.666658
211.228083	4551.138001	7.103936	-0.042164	3.669756
211.182645	4559.194571	7.108941	-0.042161	3.672849
211.614434	4567.229235	7.113946	-0.042246	3.675944
211.675107	4575.175096	7.118950	-0.042263	3.678993
211.816743	4583.226532	7.123955	-0.042294	3.682081
211.952175	4591.254209	7.128960	-0.042325	3.685158
212.290677	4599.231136	7.133965	-0.042393	3.688218
212.407349	4607.326724	7.138970	-0.042420	3.691315
212.647594	4615.318807	7.143974	-0.042470	3.694373
212.611548	4623.352931	7.148979	-0.042469	3.697437
212.877312	4631.378077	7.153984	-0.042523	3.700504
212.947142	4639.361280	7.158989	-0.042541	3.703546
213.242151	4647.436568	7.163994	-0.042602	3.706627
213.612229	4655.407901	7.168998	-0.042676	3.709668
213.642828	4663.518019	7.174003	-0.042687	3.712750
213.856873	4671.570433	7.179008	-0.042732	3.715812
214.018828	4679.527548	7.184013	-0.042767	3.718835
214.399824	4687.523338	7.189018	-0.042843	3.721875
214.390591	4695.505385	7.194022	-0.042847	3.724897
214.386806	4703.536491	7.199027	-0.042851	3.727936
214.699062	4711.594586	7.204032	-0.042915	3.730991
214.861857	4719.581248	7.209037	-0.042950	3.734012
215.012350	4727.654662	7.214042	-0.042984	3.737063
215.216228	4735.662663	7.219046	-0.043027	3.740088
215.527590	4743.650620	7.224051	-0.043090	3.743106
215.979758	4751.708535	7.229056	-0.043179	3.746151
216.672904	4759.720026	7.234061	-0.043314	3.749181
216.980612	4767.786326	7.239066	-0.043376	3.752221
217.480814	4775.780883	7.244070	-0.043475	3.755235
217.500272	4783.806744	7.249075	-0.043483	3.758248
217.805805	4791.858119	7.254080	-0.043546	3.761275
218.127758	4799.791757	7.259085	-0.043611	3.764255
218.487819	4807.862969	7.264090	-0.043683	3.767285
218.617630	4815.894755	7.269094	-0.043712	3.770293
219.155567	4823.924124	7.274099	-0.043818	3.773306
219.347790	4831.976053	7.279104	-0.043859	3.776318
219.384997	4839.938403	7.284109	-0.043871	3.779291
219.783810	4847.985815	7.289114	-0.043951	3.782301
220.044238	4855.967641	7.294118	-0.044004	3.785281
220.146161	4864.003092	7.299123	-0.044028	3.788275
220.416248	4872.061808	7.304128	-0.044084	3.791279
220.631460	4880.102570	7.309133	-0.044129	3.794272
220.889098	4888.125412	7.314138	-0.044183	3.797258
221.041371	4896.094416	7.319142	-0.044216	3.800219
221.173400	4904.098689	7.324147	-0.044246	3.803190
221.397314	4912.123292	7.329152	-0.044293	3.806168
221.538802	4920.157409	7.334157	-0.044324	3.809146
221.775622	4928.192336	7.339162	-0.044374	3.812124
221.932573	4936.201957	7.344166	-0.044408	3.815088
221.885697	4944.212747	7.349171	-0.044405	3.818046
222.134296	4952.250803	7.354176	-0.044456	3.821018
222.279777	4960.229169	7.359181	-0.044489	3.823964
222.473432	4968.313548	7.364186	-0.044530	3.826947
222.698149	4976.273637	7.369190	-0.044577	3.829883
222.859544	4984.338602	7.374195	-0.044612	3.832854
222.993946	4992.383396	7.379200	-0.044642	3.835815
223.020054	5000.358117	7.384205	-0.044653	3.838745
223.312565	5008.409904	7.389210	-0.044712	3.841707
223.826824	5016.333011	7.394214	-0.044813	3.844624
223.744986	5024.422599	7.399219	-0.044803	3.847587
223.867473	5032.466097	7.404224	-0.044831	3.850536
224.124875	5040.496396	7.409229	-0.044884	3.853480
224.395630	5048.536486	7.414234	-0.044940	3.856425
224.638622	5056.492066	7.419238	-0.044991	3.859337
224.846339	5064.563478	7.424243	-0.045034	3.862289
225.134307	5072.551171	7.429248	-0.045093	3.865209
225.341462	5080.603408	7.434253	-0.045137	3.868148
225.570270	5088.652119	7.439258	-0.045185	3.871085
225.623049	5096.895887	7.444262	-0.045200	3.874087
226.104411	5104.846503	7.449267	-0.045295	3.876988
226.401567	5112.753881	7.454272	-0.045355	3.879868
226.564229	5120.711438	7.459277	-0.045391	3.882761
226.734550	5128.718488	7.464282	-0.045428	3.885670
226.889175	5136.734176	7.469286	-0.045462	3.888580
227.259088	5144.760068	7.474291	-0.045536	3.891495
227.740075	5152.810444	7.479296	-0.045631	3.894419
227.811976	5160.800513	7.484301	-0.045649	3.897311
228.224989	5168.825362	7.489306	-0.045732	3.900220
228.502071	5176.839264	7.494310	-0.045788	3.903121
228.657756	5184.843926	7.499315	-0.045823	3.906013
228.720514	5192.894034	7.504320	-0.045840	3.908918
228.814037	5200.919119	7.509325	-0.045862	3.911813
229.240283	5208.958263	7.514330	-0.045947	3.914716
229.241220	5216.961100	7.519334	-0.045952	3.917596
229.598759	5224.959484	7.524339	-0.046024	3.920480
229.913948	5232.984314	7.529344	-0.046088	3.923369
230.124444	5240.995274	7.534349	-0.046132	3.926250
230.434691	5249.009803	7.539354	-0.046195	3.929132
230.732640	5257.042294	7.544358	-0.046256	3.932017
230.958878	5265.061742	7.549363	-0.046303	3.934895
231.130592	5273.112556	7.554368	-0.046341	3.937780
231.292981	5281.072926	7.559373	-0.046376	3.940631
231.633054	5289.091510	7.564378	-0.046445	3.943504
231.676204	5297.114962	7.569382	-0.046458	3.946372
231.951975	5305.121507	7.574387	-0.046514	3.949235
232.106089	5313.193326	7.579392	-0.046548	3.952117
232.166786	5321.248491	7.584397	-0.046565	3.954990
232.440777	5329.224698	7.589402	-0.046621	3.957836
232.474783	5337.233254	7.594406	-0.046633	3.960687
232.710484	5345.236162	7.599411	-0.046682	3.963538
233.122925	5353.267240	7.604416	-0.046764	3.966399
233.354744	5361.226732	7.609421	-0.046812	3.969230
233.644089	5369.292235	7.614426	-0.046871	3.972098
233.757558	5377.314766	7.619430	-0.046898	3.974945
233.752137	5385.383065	7.624435	-0.046902	3.977805
233.904934	5393.396853	7.629440	-0.046936	3.980645
233.996841	5401.382213	7.634445	-0.046958	3.983473
234.167595	5409.400539	7.639450	-0.046995	3.986311
234.369881	5417.444410	7.644454	-0.047038	3.989157
234.597855	5425.469057	7.649459	-0.047086	3.991995
234.928299	5433.551458	7.654464	-0.047152	3.994853
234.793710	5441.562728	7.659469	-0.047133	3.997675
235.283451	5449.552101	7.664474	-0.047229	4.000499
235.407315	5457.539068	7.669478	-0.047257	4.003313
235.426992	5465.562151	7.674483	-0.047266	4.006137
235.873575	5473.621480	7.679488	-0.047355	4.008978
236.130515	5481.611653	7.684493	-0.047408	4.011789
236.118463	5489.650648	7.689498	-0.047411	4.014612
236.252140	5497.678165	7.694502	-0.047441	4.017431
236.449184	5505.670289	7.699507	-0.047483	4.020236
236.435332	5513.721913	7.704512	-0.047485	4.023057
236.800241	5521.702869	7.709517	-0.047558	4.025857
236.948821	5529.739124	7.714522	-0.047591	4.028672
237.220483	5537.759656	7.719526	-0.047647	4.031480
237.262111	5545.895935	7.724531	-0.047660	4.034324
237.616520	5553.868018	7.729536	-0.047731	4.037113
237.876969	5561.821143	7.734541	-0.047785	4.039891
237.897461	5569.828587	7.739546	-0.047794	4.042684
238.054046	5577.808032	7.744550	-0.047829	4.045466
238.342409	5585.809909	7.749555	-0.047887	4.048257
238.279614	5593.900391	7.754560	-0.047881	4.051071
238.483861	5601.892809	7.759565	-0.047924	4.053853
238.792976	5609.931389	7.764570	-0.047987	4.056651
238.763072	5617.906040	7.769574	-0.047987	4.059419
238.877743	5625.952178	7.774579	-0.048013	4.062213
239.291557	5633.927696	7.779584	-0.048096	4.064984
239.734726	5641.944592	7.784589	-0.048183	4.067768
239.778062	5649.989725	7.789594	-0.048197	4.070555
239.848411	5658.056453	7.794598	-0.048215	4.073347
240.175281	5666.059729	7.799603	-0.048281	4.076119
240.403307	5674.047247	7.804608	-0.048329	4.078882
240.192672	5682.101169	7.809613	-0.048295	4.081661
240.731804	5690.051136	7.814618	-0.048400	4.084412
240.938001	5698.107673	7.819622	-0.048444	4.087193
241.002160	5706.079302	7.824627	-0.048461	4.089941
241.238475	5714.161148	7.829632	-0.048510	4.092727
241.345245	5722.166522	7.834637	-0.048536	4.095483
241.665711	5730.188149	7.839642	-0.048600	4.098246
242.085320	5738.199703	7.844646	-0.048684	4.101005
242.741908	5746.199580	7.849651	-0.048811	4.103761
243.209651	5754.268726	7.854656	-0.048904	4.106537
243.129906	5762.246804	7.859661	-0.048894	4.109272
243.392103	5770.336654	7.864666	-0.048948	4.112048
243.856406	5778.363419	7.869670	-0.049040	4.114803
244.026067	5786.372078	7.874675	-0.049077	4.117547
244.234373	5794.342722	7.879680	-0.049121	4.120276
244.297021	5802.334168	7.884685	-0.049137	4.123008
244.590390	5810.365451	7.889690	-0.049197	4.125755
244.713097	5818.391064	7.894694	-0.049225	4.128496
244.963415	5826.401871	7.899699	-0.049277	4.131232
245.270288	5834.489345	7.904704	-0.049340	4.133993
245.209898	5842.506632	7.909709	-0.049334	4.136723
245.459726	5850.477751	7.914714	-0.049385	4.139440
245.866797	5858.538588	7.919718	-0.049466	4.142187
245.892162	5866.486169	7.924723	-0.049476	4.144890
246.110373	5874.568214	7.929728	-0.049522	4.147638
246.477501	5882.574170	7.934733	-0.049596	4.150361
246.799843	5890.628518	7.939738	-0.049661	4.153098
246.713429	5898.648106	7.944742	-0.049650	4.155816
246.917760	5906.638962	7.949747	-0.049693	4.158526
247.086805	5914.681518	7.954752	-0.049730	4.161252
247.217646	5922.620905	7.959757	-0.049760	4.163940
247.425436	5930.686624	7.964762	-0.049804	4.166670
247.503820	5938.673364	7.969766	-0.049824	4.169371
247.519706	5946.686827	7.974771	-0.049832	4.172077
247.650005	5954.773878	7.979776	-0.049861	4.174809
247.972746	5962.759016	7.984781	-0.049927	4.177506
248.208376	5970.752313	7.989786	-0.049976	4.180203
248.251998	5978.797929	7.994790	-0.049989	4.182914
248.517486	5986.771094	7.999795	-0.050044	4.185601
248.658202	5994.800862	8.004800	-0.050075	4.188304
248.734646	6002.863020	8.009805	-0.050095	4.191015
249.028862	6010.943954	8.014810	-0.050155	4.193733
249.367137	6019.012125	8.019814	-0.050223	4.196446
249.492718	6026.905282	8.024819	-0.050251	4.199096
249.703924	6034.937706	8.029824	-0.050296	4.201792
250.134301	6042.859545	8.034829	-0.050381	4.204451
250.313784	6050.883843	8.039834	-0.050420	4.207141
250.455768	6058.925704	8.044838	-0.050452	4.209834
250.490030	6066.965791	8.049843	-0.050463	4.212523
250.898034	6075.007198	8.054848	-0.050544	4.215215
250.911122	6083.004096	8.059853	-0.050552	4.217887
250.990714	6090.997541	8.064858	-0.050572	4.220556
251.357740	6099.032484	8.069862	-0.050646	4.223240
251.424923	6107.000986	8.074867	-0.050663	4.225898
251.659298	6115.090548	8.079872	-0.050712	4.228596
251.748628	6123.063926	8.084877	-0.050734	4.231252
251.940171	6131.130433	8.089882	-0.050775	4.233938
251.971344	6139.192669	8.094886	-0.050786	4.236619
252.138179	6147.125549	8.099891	-0.050822	4.239257
252.512118	6155.191096	8.104896	-0.050897	4.241940
252.449666	6163.123648	8.109901	-0.050891	4.244572
252.662330	6171.211582	8.114906	-0.050936	4.247257
252.862273	6179.198630	8.119910	-0.050978	4.249907
252.993105	6187.260526	8.124915	-0.051008	4.252579
252.999599	6195.322465	8.129920	-0.051014	4.255248
253.293385	6203.272190	8.134925	-0.051074	4.257881
253.586178	6211.273265	8.139930	-0.051134	4.260530
253.551036	6219.337364	8.144934	-0.051133	4.263194
253.500483	6227.328426	8.149939	-0.051128	4.265833
253.942946	6235.382382	8.154944	-0.051216	4.268495
253.901428	6243.351973	8.159949	-0.051213	4.271124
254.212021	6251.462261	8.164954	-0.051277	4.273800
254.409032	6259.485899	8.169958	-0.051319	4.276445
254.160525	6267.432090	8.174963	-0.051277	4.279059
254.779261	6275.512876	8.179968	-0.051398	4.281723
254.770181	6283.436230	8.184973	-0.051401	4.284328
254.983436	6291.527055	8.189978	-0.051446	4.286989
255.080639	6299.488950	8.194982	-0.051470	4.289604
255.032947	6307.545905	8.199987	-0.051466	4.292248
255.471696	6315.553088	8.204992	-0.051553	4.294878
255.655082	6323.584890	8.209997	-0.051592	4.297513
255.596922	6331.578894	8.215002	-0.051587	4.300131
255.869498	6339.592758	8.220006	-0.051643	4.302757
255.996786	6347.589302	8.225011	-0.051672	4.305374
256.320173	6355.652069	8.230016	-0.051737	4.308013
256.217096	6363.641922	8.235021	-0.051723	4.310624
256.519624	6371.683642	8.240026	-0.051785	4.313252
256.631025	6379.735727	8.245030	-0.051811	4.315882
256.898469	6387.696370	8.250035	-0.051866	4.318480
257.013850	6395.718988	8.255040	-0.051892	4.321097
257.039225	6403.648841	8.260045	-0.051902	4.323680
257.273852	6411.763939	8.265050	-0.051951	4.326324
257.742604	6419.761893	8.270054	-0.052044	4.328930
257.995365	6427.748425	8.275059	-0.052096	4.331529
258.046490	6435.821070	8.280064	-0.052111	4.334153
258.099495	6443.820716	8.285069	-0.052126	4.336752
258.249100	6451.788517	8.290074	-0.052159	4.339340
258.649027	6459.869491	8.295078	-0.052239	4.341964
258.631233	6467.797548	8.300083	-0.052241	4.344534
259.047723	6475.862094	8.305088	-0.052323	4.347150
259.141218	6483.910276	8.310093	-0.052346	4.349757
259.250101	6491.963022	8.315098	-0.052372	4.352364
259.579157	6500.045221	8.320102	-0.052438	4.354980
259.735111	6507.958073	8.325107	-0.052472	4.357539
259.974369	6515.985186	8.330112	-0.052522	4.360134
260.055683	6523.958337	8.335117	-0.052542	4.362708
260.093314	6531.934172	8.340122	-0.052555	4.365282
260.232510	6539.994157	8.345126	-0.052586	4.367882
260.444355	6548.001441	8.350131	-0.052631	4.370464
260.786217	6556.062524	8.355136	-0.052699	4.373063
261.050929	6564.032949	8.360141	-0.052754	4.375630
261.249982	6572.064695	8.365146	-0.052796	4.378215
261.347994	6580.109893	8.370150	-0.052820	4.380802
261.603641	6588.050178	8.375155	-0.052873	4.383355
261.707882	6596.097060	8.380160	-0.052897	4.385940
261.786182	6604.145297	8.385165	-0.052917	4.388523
262.100128	6612.203021	8.390170	-0.052981	4.391109
262.199486	6620.207908	8.395174	-0.053004	4.393676
262.076587	6628.247582	8.400179	-0.052987	4.396251
262.544671	6636.234304	8.405184	-0.053079	4.398811
262.806045	6644.222440	8.410189	-0.053133	4.401368
262.956929	6652.214199	8.415194	-0.053166	4.403925
263.203180	6660.249199	8.420198	-0.053217	4.406494
263.363366	6668.218014	8.425203	-0.053252	4.409041
263.445454	6676.359027	8.430208	-0.053273	4.411640
263.437998	6684.372171	8.435213	-0.053277	4.414197
263.609856	6692.419547	8.440218	-0.053314	4.416763
263.818355	6700.372154	8.445222	-0.053358	4.419299
264.039803	6708.375309	8.450227	-0.053405	4.421849
264.053213	6716.385254	8.455232	-0.053412	4.424399
264.134441	6724.412593	8.460237	-0.053433	4.426953
264.444724	6732.439368	8.465242	-0.053496	4.429506
264.365366	6740.508833	8.470246	-0.053486	4.432070
264.632169	6748.495530	8.475251	-0.053541	4.434608
264.917673	6756.573245	8.480256	-0.053600	4.437173
265.030234	6764.466115	8.485261	-0.053626	4.439677
265.017040	6772.539525	8.490266	-0.053628	4.442236
265.495117	6780.515536	8.495270	-0.053723	4.444765
265.419636	6788.585303	8.500275	-0.053714	4.447320
265.786978	6796.567210	8.505280	-0.053787	4.449848
266.011300	6804.595097	8.510285	-0.053834	4.452388
266.160023	6812.612792	8.515290	-0.053867	4.454923
266.327005	6820.645771	8.520294	-0.053904	4.457462
266.395022	6828.615355	8.525299	-0.053922	4.459978
266.798605	6836.654798	8.530304	-0.054002	4.462517
266.860302	6844.633631	8.535309	-0.054019	4.465033
266.960083	6852.675017	8.540314	-0.054043	4.467568
267.292083	6860.724369	8.545318	-0.054110	4.470105
267.142833	6868.725200	8.550323	-0.054087	4.472624
267.476813	6876.777874	8.555328	-0.054154	4.475159
267.803189	6884.735041	8.560333	-0.054220	4.477662
267.865569	6892.743260	8.565338	-0.054237	4.480180
267.950558	6900.766720	8.570343	-0.054258	4.482700
268.040984	6908.726049	8.575347	-0.054280	4.485200
268.280327	6916.803848	8.580352	-0.054330	4.487735
268.485352	6924.791049	8.585357	-0.054374	4.490240
268.538209	6932.833056	8.590362	-0.054389	4.492761
268.756798	6940.867113	8.595367	-0.054435	4.495278
268.912762	6948.844487	8.600371	-0.054469	4.497776
269.066890	6956.912215	8.605376	-0.054503	4.500301
269.271388	6964.870262	8.610381	-0.054546	4.502790
269.564265	6972.885011	8.615386	-0.054606	4.505296
269.614330	6980.931344	8.620391	-0.054620	4.507809
269.764492	6988.919369	8.625395	-0.054654	4.510304
270.298394	6997.023964	8.630400	-0.054758	4.512834
270.314572	7005.036152	8.635405	-0.054767	4.515332
270.371259	7013.024434	8.640410	-0.054782	4.517822
270.701846	7021.006134	8.645415	-0.054849	4.520309
270.739358	7029.008488	8.650419	-0.054861	4.522800
270.951794	7037.004034	8.655424	-0.054906	4.525289
271.105232	7045.029573	8.660429	-0.054940	4.527785
271.405445	7053.036549	8.665434	-0.055001	4.530274
271.662982	7061.110655	8.670439	-0.055054	4.532782
271.582332	7069.092832	8.675443	-0.055044	4.535260
271.917774	7077.154385	8.680448	-0.055112	4.537762
271.960534	7085.109415	8.685453	-0.055125	4.540229
272.110687	7093.137725	8.690458	-0.055158	4.542718
272.145102	7101.141886	8.695463	-0.055170	4.545197
272.480273	7109.138806	8.700467	-0.055238	4.547674
272.627754	7117.174456	8.705472	-0.055270	4.550160
272.573148	7125.230676	8.710477	-0.055265	4.552652
272.732743	7133.255967	8.715482	-0.055300	4.555132
272.878998	7141.282728	8.720487	-0.055333	4.557612
273.102798	7149.227630	8.725491	-0.055380	4.560066
273.437026	7157.291835	8.730496	-0.055447	4.562554
273.592509	7165.256963	8.735501	-0.055481	4.565011
273.676342	7173.288506	8.740506	-0.055502	4.567487
273.837417	7181.347501	8.745511	-0.055537	4.569970
273.857353	7189.334319	8.750515	-0.055546	4.572429
273.956676	7197.401322	8.755520	-0.055570	4.574912
274.168948	7205.406442	8.760525	-0.055615	4.577374
274.461025	7213.417786	8.765530	-0.055675	4.579837
274.623927	7221.456238	8.770535	-0.055710	4.582307
274.823576	7229.385114	8.775539	-0.055752	4.584742
274.938970	7237.486353	8.780544	-0.055779	4.587228
275.101704	7245.438223	8.785549	-0.055815	4.589667
275.382110	7253.498103	8.790554	-0.055872	4.592138
275.672664	7261.562428	8.795559	-0.055932	4.594609
275.783464	7269.569234	8.800563	-0.055957	4.597061
275.991149	7277.514966	8.805568	-0.056001	4.599493
275.903005	7285.505056	8.810573	-0.055990	4.601938
276.137589	7293.482813	8.815578	-0.056039	4.604377
276.111140	7301.608090	8.820583	-0.056039	4.606860
276.138736	7309.606857	8.825587	-0.056050	4.609303
276.639641	7317.625196	8.830592	-0.056148	4.611750
276.774693	7325.648977	8.835597	-0.056179	4.614198
276.768741	7333.666793	8.840602	-0.056183	4.616643
277.010289	7341.698214	8.845607	-0.056233	4.619091
277.082470	7349.668263	8.850611	-0.056252	4.621518
277.284995	7357.666248	8.855616	-0.056294	4.623953
277.365648	7365.663270	8.860621	-0.056315	4.626387
277.586078	7373.695527	8.865626	-0.056361	4.628829
277.894439	7381.807253	8.870631	-0.056424	4.631295
278.112491	7389.770111	8.875635	-0.056469	4.633714
278.215651	7397.826487	8.880640	-0.056494	4.636160
278.417496	7405.756681	8.885645	-0.056537	4.638566
278.534789	7413.779431	8.890650	-0.056564	4.640999
278.720106	7421.791160	8.895655	-0.056603	4.643428
278.873384	7429.787496	8.900659	-0.056637	4.645851
278.867607	7437.829899	8.905664	-0.056641	4.648286
279.102860	7445.811227	8.910669	-0.056690	4.650702
279.460185	7453.893204	8.915674	-0.056762	4.653146
279.405848	7461.917224	8.920679	-0.056757	4.655572
279.403162	7469.930104	8.925683	-0.056762	4.657994
279.750586	7477.891632	8.930688	-0.056832	4.660398
280.060487	7485.945194	8.935693	-0.056895	4.662829
280.249088	7493.909423	8.940698	-0.056935	4.665231
280.358376	7501.973795	8.945703	-0.056961	4.667663
280.569087	7509.938244	8.950707	-0.057005	4.670063
280.664660	7518.051457	8.955712	-0.057028	4.672507
280.786511	7526.112049	8.960717	-0.057056	4.674934
281.165397	7534.081709	8.965722	-0.057132	4.677332
281.356466	7542.074328	8.970727	-0.057173	4.679735
281.301024	7550.062491	8.975731	-0.057168	4.682137
281.384837	7558.002539	8.980736	-0.057189	4.684522
281.461975	7566.105735	8.985741	-0.057208	4.686956
281.496193	7574.053731	8.990746	-0.057220	4.689341
281.651250	7582.110659	8.995751	-0.057254	4.691758
281.909524	7590.108954	9.000755	-0.057307	4.694156
282.115893	7598.198627	9.005760	-0.057351	4.696580
282.240651	7606.147082	9.010765	-0.057379	4.698960
282.575122	7614.141802	9.015770	-0.057447	4.701353
282.749326	7622.162515	9.020775	-0.057484	4.703752
282.866657	7630.167132	9.025779	-0.057512	4.706146
283.251077	7638.187343	9.030784	-0.057588	4.708542
283.521361	7646.234933	9.035789	-0.057644	4.710946
283.534808	7654.249105	9.040794	-0.057652	4.713339
283.501910	7662.285811	9.045799	-0.057651	4.715738
283.940815	7670.278272	9.050803	-0.057738	4.718121
284.042046	7678.272014	9.055808	-0.057762	4.720504
284.147172	7686.298171	9.060813	-0.057787	4.722895
284.259000	7694.318020	9.065818	-0.057813	4.725284
284.764686	7702.355076	9.070823	-0.057912	4.727675
284.762098	7710.354851	9.075827	-0.057917	4.730055
285.056030	7718.397234	9.080832	-0.057977	4.732446
285.174391	7726.429465	9.085837	-0.058004	4.734833
285.205912	7734.414472	9.090842	-0.058015	4.737205
285.266177	7742.413262	9.095847	-0.058032	4.739580
285.668919	7750.438615	9.100851	-0.058112	4.741960
285.883450	7758.449316	9.105856	-0.058157	4.744336
285.896375	7766.448242	9.110861	-0.058165	4.746707
286.161150	7774.475038	9.115866	-0.058219	4.749085
286.457104	7782.561144	9.120871	-0.058279	4.751479
286.482315	7790.530207	9.125875	-0.058289	4.753838
286.597270	7798.629884	9.130880	-0.058316	4.756234
286.898573	7806.550052	9.135885	-0.058377	4.758575
287.078180	7814.583712	9.140890	-0.058416	4.760949
287.027942	7822.552060	9.145895	-0.058412	4.763304
286.974350	7830.558138	9.150899	-0.058407	4.765668
287.485993	7838.577417	9.155904	-0.058508	4.768033
287.681074	7846.606358	9.160909	-0.058549	4.770401
287.557271	7854.687127	9.165914	-0.058531	4.772784
287.996913	7862.678656	9.170919	-0.058618	4.775137
288.117147	7870.699716	9.175923	-0.058646	4.777499
288.068352	7878.645071	9.180928	-0.058642	4.779838
288.279048	7886.748578	9.185933	-0.058687	4.782222
288.574326	7894.668401	9.190938	-0.058747	4.784550
288.884738	7902.793193	9.195943	-0.058810	4.786937
288.991665	7910.708803	9.200947	-0.058835	4.789262
289.250164	7918.769814	9.205952	-0.058888	4.791629
289.367922	7926.772199	9.210957	-0.058916	4.793977
289.373488	7934.815204	9.215962	-0.058922	4.796337
289.712428	7942.798004	9.220967	-0.058990	4.798676
289.764995	7950.765530	9.225971	-0.059005	4.801011
289.858900	7958.816488	9.230976	-0.059028	4.803369
290.007410	7966.834976	9.235981	-0.059061	4.805716
290.059057	7974.796152	9.240986	-0.059076	4.808046
290.315602	7982.876612	9.245991	-0.059129	4.810408
290.408292	7990.353943	9.250995	-0.059151	4.812594
290.825507	7995.074846	9.256000	-0.059231	4.813971
290.823537	7997.658371	9.261005	-0.059233	4.814726
290.973317	7998.921784	9.266010	-0.059262	4.815095
291.058336	7999.398739	9.271015	-0.059278	4.815234
291.131415	8000.532780	9.276019	-0.059292	4.815565
291.296730	8000.546202	9.281024	-0.059323	4.815568
291.314094	8000.510152	9.286029	-0.059326	4.815557
291.298827	8000.537688	9.291034	-0.059323	4.815565
291.389010	8000.564830	9.296039	-0.059340	4.815573
291.523990	8000.532864	9.301043	-0.059365	4.815563
291.608245	8000.554564	9.306048	-0.059381	4.815569
291.665592	8000.539482	9.311053	-0.059392	4.815564
291.685826	8000.544092	9.316058	-0.059395	4.815565
292.033022	8000.569076	9.321063	-0.059460	4.815571
291.853277	8000.538314	9.326067	-0.059426	4.815563
291.859858	8000.468954	9.331072	-0.059428	4.815542
291.949532	8000.559145	9.336077	-0.059444	4.815568
292.117138	8000.539475	9.341082	-0.059476	4.815562
292.201258	8000.562243	9.346087	-0.059491	4.815568
292.160727	8000.525234	9.351091	-0.059484	4.815557
292.369911	8000.550072	9.356096	-0.059523	4.815564
292.449327	8000.539630	9.361101	-0.059538	4.815560
292.559128	8000.523279	9.366106	-0.059558	4.815555
292.673850	8000.560448	9.371111	-0.059579	4.815565
292.825677	8000.542655	9.376115	-0.059608	4.815559
292.561743	8000.560731	9.381120	-0.059558	4.815566
292.586355	8000.564345	9.386125	-0.059563	4.815567
292.574408	8000.549185	9.391130	-0.059561	4.815562
292.861400	8000.469501	9.396135	-0.059614	4.815538
292.776005	8000.533284	9.401139	-0.059598	4.815557
292.808768	8000.565891	9.406144	-0.059605	4.815566
292.894842	8000.539528	9.411149	-0.059621	4.815558
292.727982	8000.577380	9.416154	-0.059589	4.815570
292.861072	8000.568896	9.421159	-0.059614	4.815567
292.796622	8000.538972	9.426163	-0.059602	4.815558
293.102293	8000.571821	9.431168	-0.059659	4.815567
293.154970	8000.566281	9.436173	-0.059669	4.815565
293.367230	8000.558039	9.441178	-0.059709	4.815561
293.674281	8000.488307	9.446183	-0.059766	4.815539
293.397978	8000.559618	9.451187	-0.059714	4.815562
293.585842	8000.590518	9.456192	-0.059749	4.815570
293.779218	8000.573413	9.461197	-0.059785	4.815564
293.736695	8000.483998	9.466202	-0.059777	4.815538
293.752805	8000.581527	9.471207	-0.059780	4.815566
293.583755	8000.548801	9.476211	-0.059749	4.815557
293.775343	8000.608622	9.481216	-0.059785	4.815574
293.836791	8000.477107	9.486221	-0.059796	4.815535
293.778738	8000.506073	9.491226	-0.059785	4.815544
293.922800	8000.603583	9.496231	-0.059812	4.815572
293.711001	8000.531672	9.501235	-0.059773	4.815552
293.788471	8000.553263	9.506240	-0.059787	4.815558
293.936100	8000.485166	9.511245	-0.059814	4.815537
293.980409	8000.609883	9.516250	-0.059823	4.815573
293.997780	8000.579176	9.521255	-0.059826	4.815564
294.151408	8000.548587	9.526259	-0.059855	4.815555
294.192595	8000.592023	9.531264	-0.059862	4.815567
293.957548	8000.463079	9.536269	-0.059818	4.815531
293.966286	8000.571174	9.541274	-0.059820	4.815562
294.251328	8000.599410	9.546279	-0.059873	4.815569
293.989317	8000.554455	9.551283	-0.059824	4.815557
294.040085	8000.577742	9.556288	-0.059834	4.815564
294.151207	8000.475907	9.561293	-0.059855	4.815533
294.231566	8000.547781	9.566298	-0.059870	4.815554
294.268540	8000.597560	9.571303	-0.059877	4.815568
294.274261	8000.564521	9.576307	-0.059878	4.815559
294.187207	8000.495744	9.581312	-0.059861	4.815539
294.251474	8000.576971	9.586317	-0.059873	4.815562
294.263965	8000.593210	9.591322	-0.059876	4.815567
294.456832	8000.489523	9.596327	-0.059912	4.815536
294.246586	8000.550170	9.601331	-0.059872	4.815555
294.442342	8000.601511	9.606336	-0.059909	4.815569
294.625936	8000.535078	9.611341	-0.059943	4.815548
294.640870	8000.541739	9.616346	-0.059946	4.815550
294.887033	8000.585365	9.621351	-0.059992	4.815562
294.574713	8000.572709	9.626355	-0.059934	4.815560
294.639732	8000.506450	9.631360	-0.059946	4.815540
294.520318	8000.566465	9.636365	-0.059923	4.815558
294.739678	8000.595751	9.641370	-0.059964	4.815566
294.777396	8000.507663	9.646375	-0.059971	4.815540
294.598807	8000.580592	9.651379	-0.059938	4.815562
294.544335	8000.589310	9.656384	-0.059928	4.815565
294.577244	8000.490454	9.661389	-0.059934	4.815536
294.694964	8000.516988	9.666394	-0.059956	4.815543
294.684188	8000.496502	9.671399	-0.059954	4.815537
294.575758	8000.591970	9.676403	-0.059934	4.815565
294.907936	8000.596405	9.681408	-0.059996	4.815565
294.905113	8000.609185	9.686413	-0.059995	4.815569
294.925216	8000.494083	9.691418	-0.059999	4.815535
294.779268	8000.604963	9.696423	-0.059972	4.815568
294.861192	8000.566773	9.701427	-0.059987	4.815557
294.758360	8000.537281	9.706432	-0.059968	4.815548
294.806909	8000.483575	9.711437	-0.059977	4.815532
294.970743	8000.598518	9.716442	-0.060007	4.815565
294.999696	8000.499595	9.721447	-0.060013	4.815536
295.096121	8000.599527	9.726451	-0.060031	4.815565
295.179620	8000.507921	9.731456	-0.060046	4.815538
294.952706	8000.600358	9.736461	-0.060004	4.815566
295.115334	8000.490824	9.741466	-0.060034	4.815533
295.265692	8000.616234	9.746471	-0.060062	4.815569
294.980332	8000.580509	9.751475	-0.060009	4.815560
294.975716	8000.499201	9.756480	-0.060008	4.815536
295.102481	8000.576121	9.761485	-0.060032	4.815558
295.123943	8000.589303	9.766490	-0.060036	4.815562
295.036717	8000.502351	9.771495	-0.060020	4.815537
295.296584	8000.590027	9.776499	-0.060068	4.815561
295.344538	8000.504245	9.781504	-0.060077	4.815536
295.309815	8000.604142	9.786509	-0.060071	4.815565
295.075352	8000.502993	9.791514	-0.060027	4.815537
295.220192	8000.497911	9.796519	-0.060054	4.815535
295.223428	8000.575991	9.801523	-0.060055	4.815557
295.118520	8000.496227	9.806528	-0.060035	4.815535
295.202790	8000.603440	9.811533	-0.060051	4.815566
295.308923	8000.497245	9.816538	-0.060070	4.815534
295.099355	8000.618829	9.821543	-0.060031	4.815571
295.360236	8000.581467	9.826547	-0.060080	4.815558
295.546539	8000.511872	9.831552	-0.060115	4.815537
295.473598	8000.497838	9.836557	-0.060101	4.815533
295.318916	8000.626744	9.841562	-0.060072	4.815572
295.329041	8000.517889	9.846567	-0.060074	4.815540
295.428670	8000.585810	9.851571	-0.060093	4.815559
295.257465	8000.607557	9.856576	-0.060061	4.815567
295.541482	8000.517136	9.861581	-0.060114	4.815539
295.566109	8000.501511	9.866586	-0.060118	4.815534
295.508060	8000.529409	9.871591	-0.060108	4.815542
295.492441	8000.590075	9.876595	-0.060105	4.815560
295.708013	8000.616095	9.881600	-0.060145	4.815567
295.610758	8000.497978	9.886605	-0.060127	4.815533
295.485094	8000.592093	9.891610	-0.060103	4.815561
295.777206	8000.509288	9.896615	-0.060158	4.815535
295.523676	8000.593802	9.901619	-0.060111	4.815561
295.475132	8000.607962	9.906624	-0.060102	4.815566
295.693312	8000.584857	9.911629	-0.060142	4.815558
295.527635	8000.591731	9.916634	-0.060111	4.815561
295.621755	8000.519540	9.921639	-0.060129	4.815539
295.596750	8000.597153	9.926643	-0.060124	4.815562
295.688797	8000.600817	9.931648	-0.060141	4.815562
295.693462	8000.495077	9.936653	-0.060142	4.815532
295.549319	8000.599575	9.941658	-0.060115	4.815563
295.637383	8000.505906	9.946663	-0.060132	4.815535
295.569184	8000.581734	9.951667	-0.060119	4.815557
295.572177	8000.609575	9.956672	-0.060120	4.815566
295.601093	8000.468965	9.961677	-0.060125	4.815524
295.666748	8000.602592	9.966682	-0.060137	4.815563
295.733160	8000.610107	9.971687	-0.060150	4.815565
295.483259	8000.563211	9.976691	-0.060103	4.815552
295.741031	8000.516178	9.981696	-0.060151	4.815537
295.654617	8000.601324	9.986701	-0.060135	4.815563
295.596863	8000.604643	9.991706	-0.060124	4.815564
295.687765	8000.508883	9.996711	-0.060141	4.815536
295.770471	8000.606452	10.001715	-0.060157	4.815564
295.910237	8000.621596	10.006720	-0.060183	4.815567
295.960686	8000.518752	10.011725	-0.060192	4.815537
295.737099	8000.618727	10.016730	-0.060150	4.815567
295.869878	8000.511904	10.021735	-0.060175	4.815536
295.804729	8000.584576	10.026739	-0.060163	4.815557
295.843787	8000.607670	10.031744	-0.060170	4.815564
295.980114	8000.505181	10.036749	-0.060196	4.815533
295.828852	8000.495193	10.041754	-0.060167	4.815531
295.933204	8000.598465	10.046759	-0.060187	4.815561
295.856311	8000.568331	10.051763	-0.060173	4.815552
295.848364	8000.495517	10.056768	-0.060171	4.815531
295.891318	8000.595634	10.061773	-0.060179	4.815560
295.871344	8000.598510	10.066778	-0.060175	4.815561
296.027363	8000.505967	10.071783	-0.060204	4.815533
295.990177	8000.568415	10.076787	-0.060198	4.815552
296.070387	8000.623188	10.081792	-0.060213	4.815567
296.099022	8000.495399	10.086797	-0.060218	4.815530
295.910093	8000.603430	10.091802	-0.060183	4.815562
296.053823	8000.601538	10.096807	-0.060209	4.815561
296.179113	8000.515967	10.101811	-0.060233	4.815535
296.259704	8000.581436	10.106816	-0.060248	4.815554
296.260859	8000.602833	10.111821	-0.060248	4.815560
295.941406	8000.509891	10.116826	-0.060188	4.815535
296.019296	8000.516527	10.121831	-0.060203	4.815536
296.128370	8000.527955	10.126835	-0.060223	4.815539
296.056571	8000.502182	10.131840	-0.060210	4.815532
296.264636	8000.622138	10.136845	-0.060249	4.815566
296.024133	8000.510196	10.141850	-0.060204	4.815534
295.902009	8000.535963	10.146855	-0.060181	4.815542
296.041311	8000.616300	10.151859	-0.060207	4.815565
296.269222	8000.522810	10.156864	-0.060250	4.815537
296.019064	8000.512251	10.161869	-0.060203	4.815535
295.966777	8000.510316	10.166874	-0.060193	4.815535
296.098168	8000.538147	10.171879	-0.060218	4.815542
295.906129	8000.486866	10.176883	-0.060182	4.815528
295.912284	8000.621646	10.181888	-0.060183	4.815567
295.959586	8000.602122	10.186893	-0.060192	4.815562
296.067950	8000.502376	10.191898	-0.060212	4.815532
296.144874	8000.597712	10.196903	-0.060227	4.815559
296.262073	8000.578278	10.201907	-0.060248	4.815553
295.979640	8000.604594	10.206912	-0.060196	4.815562
296.214867	8000.524052	10.211917	-0.060240	4.815537
296.149613	8000.604206	10.216922	-0.060227	4.815561
296.132838	8000.508798	10.221927	-0.060224	4.815533
296.072723	8000.595450	10.226931	-0.060213	4.815559
296.305963	8000.521289	10.231936	-0.060256	4.815536
296.267288	8000.605089	10.236941	-0.060249	4.815561
296.259086	8000.522650	10.241946	-0.060248	4.815537
296.206437	8000.624390	10.246951	-0.060238	4.815567
296.205208	8000.593373	10.251955	-0.060238	4.815558
296.315364	8000.378218	10.256960	-0.060258	4.815494
296.242944	8000.612170	10.261965	-0.060245	4.815563
296.019839	8000.611679	10.266970	-0.060203	4.815564
296.456044	8000.513091	10.271975	-0.060284	4.815533
296.247124	8000.569486	10.276979	-0.060246	4.815551
296.217254	8000.562578	10.281984	-0.060240	4.815549
296.220456	8000.418334	10.286989	-0.060241	4.815507
296.197854	8000.565464	10.291994	-0.060236	4.815550
296.295122	8000.477291	10.296999	-0.060255	4.815523
296.216777	8000.607464	10.302003	-0.060240	4.815562
296.404431	8000.623402	10.307008	-0.060275	4.815566
296.238824	8000.497737	10.312013	-0.060244	4.815530
296.209696	8000.615899	10.317018	-0.060239	4.815564
296.470525	8000.526162	10.322023	-0.060287	4.815537
296.313994	8000.606941	10.327027	-0.060258	4.815561
296.176747	8000.507398	10.332032	-0.060233	4.815533
296.283857	8000.518794	10.337037	-0.060252	4.815536
296.302845	8000.602482	10.342042	-0.060256	4.815560
296.186806	8000.521462	10.347047	-0.060234	4.815537
296.186663	8000.569559	10.352051	-0.060234	4.815551
296.402209	8000.453419	10.357056	-0.060275	4.815516
296.290310	8000.507146	10.362061	-0.060254	4.815532
296.338626	8000.527187	10.367066	-0.060263	4.815538
296.628860	8000.629267	10.372071	-0.060317	4.815566
296.431952	8000.502013	10.377075	-0.060280	4.815530
296.340752	8000.614871	10.382080	-0.060263	4.815563
296.466925	8000.516489	10.387085	-0.060287	4.815534
296.536753	8000.513371	10.392090	-0.060300	4.815533
296.442971	8000.518230	10.397095	-0.060282	4.815535
296.202865	8000.517457	10.402099	-0.060237	4.815536
296.263408	8000.622143	10.407104	-0.060249	4.815566
296.270985	8000.515381	10.412109	-0.060250	4.815535
296.019737	8000.591382	10.417114	-0.060203	4.815558
296.225523	8000.509284	10.422119	-0.060242	4.815533
296.233523	8000.581032	10.427123	-0.060243	4.815554
296.230996	8000.591679	10.432128	-0.060243	4.815557
296.206893	8000.598762	10.437133	-0.060238	4.815559
296.336742	8000.558160	10.442138	-0.060262	4.815547
296.327437	8000.603968	10.447143	-0.060261	4.815560
296.312986	8000.593040	10.452147	-0.060258	4.815557
296.438295	8000.487161	10.457152	-0.060281	4.815526
296.417030	8000.596903	10.462157	-0.060277	4.815558
296.259091	8000.570770	10.467162	-0.060248	4.815551
296.587561	8000.631798	10.472167	-0.060309	4.815567
296.398306	8000.585906	10.477171	-0.060274	4.815555
296.262422	8000.523796	10.482176	-0.060249	4.815537
296.347987	8000.620345	10.487181	-0.060265	4.815565
296.292785	8000.575607	10.492186	-0.060254	4.815552
296.429620	8000.537258	10.497191	-0.060280	4.815540
296.320041	8000.489480	10.502195	-0.060259	4.815527
296.434299	8000.599332	10.507200	-0.060281	4.815558
296.606419	8000.607530	10.512205	-0.060313	4.815560
296.437130	8000.575864	10.517210	-0.060281	4.815552
296.491071	8000.620583	10.522215	-0.060291	4.815564
296.343589	8000.481322	10.527219	-0.060264	4.815524
296.432152	8000.619607	10.532224	-0.060280	4.815564
296.408304	8000.509118	10.537229	-0.060276	4.815532
296.341590	8000.617038	10.542234	-0.060264	4.815564
296.401568	8000.531453	10.547239	-0.060275	4.815539
296.348896	8000.497445	10.552243	-0.060265	4.815529
296.389103	8000.514145	10.557248	-0.060272	4.815534
296.527462	8000.609432	10.562253	-0.060298	4.815561
296.226845	8000.569176	10.567258	-0.060242	4.815551
296.440086	8000.595158	10.572263	-0.060282	4.815557
296.620610	8000.582118	10.577267	-0.060315	4.815552
296.418362	8000.528528	10.582272	-0.060278	4.815538
296.366274	8000.612107	10.587277	-0.060268	4.815562
296.669957	8000.524149	10.592282	-0.060325	4.815535
296.518104	8000.608212	10.597287	-0.060296	4.815561
296.244226	8000.585500	10.602291	-0.060245	4.815555
296.518172	8000.520565	10.607296	-0.060296	4.815535
296.658717	8000.635129	10.612301	-0.060323	4.815568
296.549295	8000.602317	10.617306	-0.060302	4.815559
296.537086	8000.527293	10.622311	-0.060300	4.815537
296.519188	8000.505620	10.627315	-0.060297	4.815531
296.431686	8000.617471	10.632320	-0.060280	4.815564
296.545903	8000.477204	10.637325	-0.060302	4.815522
296.553293	8000.625901	10.642330	-0.060303	4.815566
296.668303	8000.528402	10.647335	-0.060324	4.815537
296.512026	8000.618805	10.652339	-0.060295	4.815564
296.537241	8000.510197	10.657344	-0.060300	4.815532
296.715056	8000.492837	10.662349	-0.060333	4.815526
296.495656	8000.511646	10.667354	-0.060292	4.815532
296.637642	8000.521483	10.672359	-0.060319	4.815535
296.611814	8000.609773	10.677363	-0.060314	4.815561
296.729949	8000.532634	10.682368	-0.060336	4.815537
296.787053	8000.519686	10.687373	-0.060347	4.815533
296.769953	8000.607052	10.692378	-0.060343	4.815559
296.873784	8000.537158	10.697383	-0.060363	4.815538
296.866571	8000.516730	10.702387	-0.060361	4.815532
296.743699	8000.561724	10.707392	-0.060339	4.815546
296.783678	8000.516425	10.712397	-0.060346	4.815532
296.557684	8000.600328	10.717402	-0.060304	4.815558
296.481891	8000.525319	10.722407	-0.060290	4.815537
296.584327	8000.562290	10.727411	-0.060309	4.815547
296.546494	8000.532804	10.732416	-0.060302	4.815538
296.590110	8000.615832	10.737421	-0.060310	4.815562
296.484906	8000.583090	10.742426	-0.060290	4.815553
296.729736	8000.520879	10.747431	-0.060336	4.815534
296.663465	8000.614911	10.752435	-0.060324	4.815562
296.592342	8000.537842	10.757440	-0.060310	4.815540
296.722588	8000.511142	10.762445	-0.060335	4.815531
296.949530	8000.604692	10.767450	-0.060377	4.815557
296.842986	8000.513139	10.772455	-0.060357	4.815531
296.718568	8000.603001	10.777459	-0.060334	4.815558
296.736901	8000.522070	10.782464	-0.060337	4.815534
296.619665	8000.513713	10.787469	-0.060315	4.815532
296.659258	8000.608432	10.792474	-0.060323	4.815560
296.730299	8000.505928	10.797479	-0.060336	4.815530
296.439225	8000.620818	10.802483	-0.060282	4.815565
296.512361	8000.510867	10.807488	-0.060296	4.815532
296.748045	8000.516913	10.812493	-0.060339	4.815533
296.580814	8000.593238	10.817498	-0.060308	4.815556
296.612271	8000.490078	10.822503	-0.060314	4.815526
296.540420	8000.606465	10.827507	-0.060301	4.815560
296.623661	8000.603570	10.832512	-0.060316	4.815559
296.681341	8000.515809	10.837517	-0.060327	4.815533
296.599276	8000.503760	10.842522	-0.060312	4.815530
296.695978	8000.517122	10.847527	-0.060330	4.815533
296.857143	8000.608512	10.852531	-0.060360	4.815559
296.834257	8000.492693	10.857536	-0.060355	4.815525
296.706790	8000.615640	10.862541	-0.060332	4.815562
296.704906	8000.539718	10.867546	-0.060331	4.815540
296.866430	8000.580877	10.872551	-0.060362	4.815551
296.811105	8000.489104	10.877555	-0.060351	4.815524
296.839879	8000.538750	10.882560	-0.060357	4.815539
296.696847	8000.520346	10.887565	-0.060330	4.815534
296.565970	8000.614377	10.892570	-0.060306	4.815562
296.792238	8000.533686	10.897575	-0.060348	4.815537
296.762821	8000.591988	10.902579	-0.060342	4.815555
296.701422	8000.603797	10.907584	-0.060331	4.815558
296.828449	8000.501153	10.912589	-0.060354	4.815528
296.872263	8000.609838	10.917594	-0.060363	4.815559
296.814902	8000.500929	10.922599	-0.060352	4.815528
296.792828	8000.489875	10.927603	-0.060348	4.815525
296.816662	8000.513786	10.932608	-0.060352	4.815532
296.886887	8000.614357	10.937613	-0.060365	4.815561
296.686483	8000.497733	10.942618	-0.060328	4.815528
296.954977	8000.620832	10.947623	-0.060378	4.815562
296.944340	8000.605691	10.952627	-0.060376	4.815558
296.819585	8000.507423	10.957632	-0.060353	4.815530
296.890020	8000.630445	10.962637	-0.060366	4.815565
296.838021	8000.606068	10.967642	-0.060356	4.815558
296.818623	8000.526649	10.972647	-0.060353	4.815535
296.713445	8000.486425	10.977651	-0.060333	4.815524
296.871051	8000.629064	10.982656	-0.060363	4.815565
296.739516	8000.514649	10.987661	-0.060338	4.815532
296.674819	8000.517853	10.992666	-0.060326	4.815533
296.899377	8000.529059	10.997671	-0.060368	4.815536
296.929251	8000.616135	11.002675	-0.060373	4.815561
296.799456	8000.513507	11.007680	-0.060349	4.815532
296.867918	8000.601223	11.012685	-0.060362	4.815557
296.935246	8000.571342	11.017690	-0.060375	4.815548
296.891994	8000.600554	11.022695	-0.060366	4.815557
297.059080	8000.519952	11.027699	-0.060398	4.815532
297.174195	8000.624475	11.032704	-0.060419	4.815562
296.944522	8000.494537	11.037709	-0.060376	4.815525
296.869643	8000.600185	11.042714	-0.060362	4.815557
297.082460	8000.537443	11.047719	-0.060402	4.815537
296.904107	8000.490662	11.052723	-0.060369	4.815524
296.767156	8000.598487	11.057728	-0.060343	4.815557
297.078665	8000.400564	11.062733	-0.060401	4.815497
297.218105	8000.418909	11.067738	-0.060427	4.815502
297.020318	8000.640098	11.072743	-0.060390	4.815567
296.945409	8000.499900	11.077747	-0.060376	4.815527
297.050056	8000.526220	11.082752	-0.060396	4.815534
297.167690	8000.637199	11.087757	-0.060418	4.815566
296.992944	8000.487863	11.092762	-0.060385	4.815523
297.234111	8000.521791	11.097767	-0.060430	4.815532
297.039093	8000.498249	11.102771	-0.060394	4.815526
296.980209	8000.599887	11.107776	-0.060383	4.815556
297.130498	8000.632309	11.112781	-0.060411	4.815565
297.149815	8000.517189	11.117786	-0.060415	4.815531
297.260159	8000.540397	11.122791	-0.060435	4.815537
296.924250	8000.620339	11.127795	-0.060373	4.815562
297.005321	8000.616339	11.132800	-0.060388	4.815561
297.099063	8000.487489	11.137805	-0.060405	4.815523
297.075024	8000.596118	11.142810	-0.060401	4.815554
297.218244	8000.515119	11.147815	-0.060427	4.815530
297.215256	8000.500106	11.152819	-0.060427	4.815526
297.020018	8000.524660	11.157824	-0.060390	4.815534
297.007734	8000.553317	11.162829	-0.060388	4.815542
296.996741	8000.557411	11.167834	-0.060386	4.815543
297.088537	8000.453113	11.172839	-0.060403	4.815513
297.033545	8000.602916	11.177843	-0.060393	4.815557
297.133802	8000.610992	11.182848	-0.060412	4.815558
297.258999	8000.507248	11.187853	-0.060435	4.815528
297.058023	8000.516742	11.192858	-0.060398	4.815531
297.170709	8000.619088	11.197863	-0.060419	4.815561
297.285315	8000.494859	11.202867	-0.060440	4.815524
297.359930	8000.538853	11.207872	-0.060454	4.815536
297.169837	8000.410640	11.212877	-0.060418	4.815500
297.071818	8000.600347	11.217882	-0.060400	4.815556
297.086483	8000.549284	11.222887	-0.060403	4.815541
297.163721	8000.472536	11.227891	-0.060417	4.815518
297.018552	8000.630464	11.232896	-0.060390	4.815565
297.227403	8000.428699	11.237901	-0.060429	4.815505
297.014044	8000.607943	11.242906	-0.060389	4.815558
297.101150	8000.638248	11.247911	-0.060406	4.815567
296.908303	8000.511059	11.252915	-0.060370	4.815530
297.134582	8000.614219	11.257920	-0.060412	4.815559
297.234948	8000.531440	11.262925	-0.060431	4.815535
297.182389	8000.607530	11.267930	-0.060421	4.815557
297.302428	8000.442773	11.272935	-0.060443	4.815508
297.064885	8000.517933	11.277939	-0.060399	4.815532
297.055423	8000.616115	11.282944	-0.060397	4.815560
297.089298	8000.518339	11.287949	-0.060403	4.815532
297.009374	8000.620697	11.292954	-0.060389	4.815562
296.957660	8000.530052	11.297959	-0.060379	4.815536
297.054594	8000.529522	11.302963	-0.060397	4.815535
296.984483	8000.612803	11.307968	-0.060384	4.815560
296.958217	8000.504410	11.312973	-0.060379	4.815528
296.866179	8000.602291	11.317978	-0.060362	4.815557
297.064982	8000.539317	11.322983	-0.060399	4.815538
296.878519	8000.526605	11.327987	-0.060364	4.815535
296.930454	8000.605496	11.332992	-0.060374	4.815558
297.067612	8000.624873	11.337997	-0.060400	4.815563
297.118679	8000.555173	11.343002	-0.060409	4.815542
296.925170	8000.549827	11.348007	-0.060373	4.815542
296.948959	8000.511742	11.353011	-0.060377	4.815530
297.101157	8000.537782	11.358016	-0.060406	4.815537
297.200191	8000.528735	11.363021	-0.060424	4.815534
296.942114	8000.617450	11.368026	-0.060376	4.815561
297.056873	8000.614009	11.373031	-0.060398	4.815560
297.213708	8000.610197	11.378035	-0.060427	4.815558
297.206428	8000.511738	11.383040	-0.060425	4.815529
297.000482	8000.391815	11.388045	-0.060387	4.815495
296.906565	8000.524938	11.393050	-0.060370	4.815534
296.844174	8000.513215	11.398055	-0.060358	4.815531
296.900982	8000.502400	11.403059	-0.060368	4.815528
296.983164	8000.629893	11.408064	-0.060384	4.815565
296.931237	8000.517867	11.413069	-0.060374	4.815532
296.836968	8000.609298	11.418074	-0.060357	4.815559
296.925897	8000.627875	11.423079	-0.060373	4.815564
296.901847	8000.522726	11.428083	-0.060369	4.815534
296.904855	8000.523845	11.433088	-0.060369	4.815534
297.098343	8000.534536	11.438093	-0.060405	4.815536
297.222878	8000.605011	11.443098	-0.060429	4.815556
297.232722	8000.516456	11.448103	-0.060430	4.815530
297.189855	8000.487954	11.453107	-0.060422	4.815522
297.105201	8000.512204	11.458112	-0.060407	4.815530
296.963269	8000.628499	11.463117	-0.060380	4.815564
297.021503	8000.599536	11.468122	-0.060391	4.815556
297.253284	8000.515730	11.473127	-0.060434	4.815530
297.029311	8000.591115	11.478131	-0.060393	4.815553
296.981182	8000.598869	11.483136	-0.060384	4.815556
297.283151	8000.521571	11.488141	-0.060440	4.815532
297.212037	8000.584527	11.493146	-0.060427	4.815550
297.191838	8000.636568	11.498151	-0.060423	4.815566
297.158540	8000.501335	11.503155	-0.060417	4.815526
297.142316	8000.630403	11.508160	-0.060414	4.815564
297.203809	8000.515982	11.513165	-0.060425	4.815530
297.184508	8000.618277	11.518170	-0.060421	4.815560
297.285144	8000.630636	11.523175	-0.060440	4.815563
297.250787	8000.610826	11.528179	-0.060434	4.815558
297.126085	8000.520040	11.533184	-0.060411	4.815532
297.401165	8000.512844	11.538189	-0.060462	4.815528
297.513458	8000.622666	11.543194	-0.060483	4.815560
297.238615	8000.516563	11.548199	-0.060432	4.815530
297.243254	8000.620324	11.553203	-0.060432	4.815561
297.254139	8000.518959	11.558208	-0.060434	4.815531
297.407779	8000.515094	11.563213	-0.060463	4.815529
297.196560	8000.614206	11.568218	-0.060424	4.815559
297.276275	8000.525741	11.573223	-0.060439	4.815533
297.243202	8000.528399	11.578227	-0.060432	4.815534
297.140517	8000.599382	11.583232	-0.060413	4.815555
297.183201	8000.514579	11.588237	-0.060421	4.815530
297.225089	8000.597579	11.593242	-0.060429	4.815554
297.190792	8000.628009	11.598247	-0.060423	4.815563
297.149635	8000.500128	11.603251	-0.060415	4.815526
297.271677	8000.526737	11.608256	-0.060438	4.815533
297.295605	8000.523927	11.613261	-0.060442	4.815532
297.213069	8000.624105	11.618266	-0.060427	4.815562
297.155296	8000.535497	11.623271	-0.060416	4.815536
297.124648	8000.601261	11.628275	-0.060410	4.815556
296.991885	8000.590509	11.633280	-0.060386	4.815553
297.347965	8000.524798	11.638285	-0.060452	4.815532
297.408729	8000.611318	11.643290	-0.060463	4.815557
297.391895	8000.533010	11.648295	-0.060460	4.815534
297.279707	8000.504427	11.653299	-0.060439	4.815527
297.283351	8000.623136	11.658304	-0.060440	4.815561
297.441212	8000.550931	11.663309	-0.060469	4.815539
297.114809	8000.527348	11.668314	-0.060409	4.815534
297.227357	8000.534559	11.673319	-0.060430	4.815536
297.253870	8000.474072	11.678323	-0.060434	4.815518
297.074376	8000.633568	11.683328	-0.060401	4.815565
297.278792	8000.538620	11.688333	-0.060439	4.815537
297.400575	8000.392063	11.693338	-0.060462	4.815493
297.477671	8000.520541	11.698343	-0.060476	4.815530
297.313697	8000.534924	11.703347	-0.060446	4.815535
297.550129	8000.529226	11.708352	-0.060490	4.815532
297.480964	8000.529148	11.713357	-0.060477	4.815533
297.484500	8000.506760	11.718362	-0.060477	4.815526
297.419193	8000.639291	11.723367	-0.060465	4.815565
297.343588	8000.510838	11.728371	-0.060451	4.815528
297.459309	8000.509551	11.733376	-0.060473	4.815527
297.530233	8000.275570	11.738381	-0.060486	4.815459
297.342001	8000.603807	11.743386	-0.060451	4.815555
297.500741	8000.407625	11.748391	-0.060480	4.815497
297.284555	8000.353803	11.753395	-0.060440	4.815483
297.313128	8000.528507	11.758400	-0.060446	4.815533
297.538722	8000.527973	11.763405	-0.060488	4.815532
297.357671	8000.518557	11.768410	-0.060454	4.815530
297.181137	8000.618245	11.773415	-0.060421	4.815560
297.404545	8000.493682	11.778419	-0.060463	4.815523
297.276206	8000.626236	11.783424	-0.060439	4.815562
297.263622	8000.628165	11.788429	-0.060436	4.815563
297.215299	8000.556817	11.793434	-0.060427	4.815542
297.219126	8000.510918	11.798439	-0.060428	4.815529
297.311502	8000.615065	11.803443	-0.060445	4.815559
297.219842	8000.627441	11.808448	-0.060428	4.815563
297.466906	8000.533200	11.813453	-0.060474	4.815534
297.234045	8000.618057	11.818458	-0.060431	4.815560
297.167990	8000.522899	11.823463	-0.060419	4.815532
297.281997	8000.457450	11.828467	-0.060440	4.815513
297.346470	8000.577167	11.833472	-0.060452	4.815547
297.283267	8000.542983	11.838477	-0.060440	4.815538
297.250621	8000.506100	11.843482	-0.060434	4.815527
297.388351	8000.541520	11.848487	-0.060460	4.815537
297.301466	8000.506944	11.853491	-0.060444	4.815527
297.167318	8000.517547	11.858496	-0.060419	4.815531
297.404222	8000.511856	11.863501	-0.060463	4.815528
297.349473	8000.502397	11.868506	-0.060452	4.815526
297.331291	8000.532025	11.873511	-0.060449	4.815534
297.422503	8000.429855	11.878515	-0.060466	4.815504
297.261118	8000.617443	11.883520	-0.060436	4.815560
297.295128	8000.406366	11.888525	-0.060442	4.815498
297.330571	8000.489259	11.893530	-0.060449	4.815522
297.357309	8000.529252	11.898535	-0.060454	4.815533
297.415030	8000.631756	11.903539	-0.060465	4.815563
297.274008	8000.510769	11.908544	-0.060438	4.815528
297.631660	8000.647108	11.913549	-0.060505	4.815567
297.514750	8000.530796	11.918554	-0.060483	4.815533
297.257586	8000.508360	11.923559	-0.060435	4.815528
297.532557	8000.524679	11.928563	-0.060487	4.815531
297.568333	8000.534893	11.933568	-0.060493	4.815534
297.511440	8000.531812	11.938573	-0.060483	4.815533
297.382307	8000.606632	11.943578	-0.060459	4.815556
297.470016	8000.636948	11.948583	-0.060475	4.815564
297.608192	8000.500282	11.953587	-0.060501	4.815524
297.297882	8000.594544	11.958592	-0.060443	4.815553
297.331532	8000.538451	11.963597	-0.060449	4.815536
297.581392	8000.513734	11.968602	-0.060496	4.815528
297.613635	8000.522821	11.973607	-0.060502	4.815530
297.657364	8000.528891	11.978611	-0.060510	4.815532
297.628303	8000.612854	11.983616	-0.060505	4.815557
297.438853	8000.637503	11.988621	-0.060469	4.815565
297.441632	8000.509281	11.993626	-0.060470	4.815527
297.513706	8000.635539	11.998631	-0.060483	4.815564
297.593803	8000.520357	12.003635	-0.060498	4.815530
297.473109	8000.541872	12.008640	-0.060476	4.815537
297.631662	8000.623601	12.013645	-0.060505	4.815560
297.685248	8000.605250	12.018650	-0.060515	4.815554
297.380050	8000.518952	12.023655	-0.060458	4.815530
297.441203	8000.516760	12.028659	-0.060470	4.815529
297.554402	8000.495121	12.033664	-0.060491	4.815523
297.688989	8000.508043	12.038669	-0.060516	4.815526
297.373477	8000.621459	12.043674	-0.060457	4.815560
297.693039	8000.435426	12.048679	-0.060517	4.815504
297.895045	8000.362884	12.053683	-0.060554	4.815482
297.552453	8000.518607	12.058688	-0.060490	4.815529
297.582020	8000.513754	12.063693	-0.060496	4.815528
297.836525	8000.636625	12.068698	-0.060543	4.815562
297.583979	8000.522338	12.073703	-0.060496	4.815530
297.439404	8000.517803	12.078707	-0.060469	4.815530
297.508413	8000.614081	12.083712	-0.060482	4.815557
297.785353	8000.547058	12.088717	-0.060534	4.815537
297.740735	8000.592281	12.093722	-0.060526	4.815550
297.801484	8000.525948	12.098727	-0.060537	4.815530
298.019552	8000.557358	12.103731	-0.060578	4.815538
297.857317	8000.471292	12.108736	-0.060547	4.815514
297.732922	8000.390130	12.113741	-0.060524	4.815491
297.769481	8000.521143	12.118746	-0.060531	4.815529
297.724286	8000.611252	12.123751	-0.060523	4.815556
297.739434	8000.527059	12.128755	-0.060525	4.815531
297.603815	8000.493812	12.133760	-0.060500	4.815522
297.886732	8000.523090	12.138765	-0.060553	4.815529
297.696186	8000.509241	12.143770	-0.060517	4.815526
297.468938	8000.375067	12.148775	-0.060475	4.815488
297.771750	8000.408949	12.153779	-0.060531	4.815496
297.590280	8000.519244	12.158784	-0.060498	4.815529
297.743204	8000.427717	12.163789	-0.060526	4.815502
297.587373	8000.630363	12.168794	-0.060497	4.815562
297.577892	8000.524384	12.173799	-0.060495	4.815531
297.597182	8000.506533	12.178803	-0.060499	4.815526
297.677527	8000.530313	12.183808	-0.060514	4.815532
297.800819	8000.529152	12.188813	-0.060537	4.815531
297.561947	8000.609634	12.193818	-0.060492	4.815556
297.696740	8000.533840	12.198823	-0.060517	4.815533
297.772874	8000.615272	12.203827	-0.060532	4.815557
297.689952	8000.563658	12.208832	-0.060516	4.815542
297.862195	8000.588963	12.213837	-0.060548	4.815548
297.831490	8000.438806	12.218842	-0.060543	4.815505
297.891656	8000.554178	12.223847	-0.060554	4.815538
297.725952	8000.553568	12.228851	-0.060523	4.815539
297.530171	8000.523598	12.233856	-0.060487	4.815531
297.751371	8000.513372	12.238861	-0.060528	4.815527
297.775303	8000.531941	12.243866	-0.060532	4.815532
297.872207	8000.614786	12.248871	-0.060550	4.815556
297.903226	8000.374796	12.253875	-0.060556	4.815486
297.826768	8000.624722	12.258880	-0.060542	4.815559
297.806883	8000.407404	12.263885	-0.060538	4.815496
297.960043	8000.517904	12.268890	-0.060567	4.815527
297.799182	8000.510961	12.273895	-0.060537	4.815526
297.865309	8000.502438	12.278899	-0.060549	4.815523
297.563146	8000.634248	12.283904	-0.060493	4.815563
297.785454	8000.517148	12.288909	-0.060534	4.815528
297.585313	8000.452902	12.293914	-0.060497	4.815510
297.626145	8000.478164	12.298919	-0.060504	4.815517
297.888771	8000.511381	12.303923	-0.060553	4.815526
297.563506	8000.619291	12.308928	-0.060493	4.815559
297.736006	8000.361339	12.313933	-0.060525	4.815483
297.906127	8000.528773	12.318938	-0.060557	4.815531
297.709010	8000.521228	12.323943	-0.060520	4.815529
297.899856	8000.411089	12.328947	-0.060555	4.815496
297.588000	8000.625044	12.333952	-0.060497	4.815560
297.760292	8000.531700	12.338957	-0.060529	4.815532
297.788983	8000.537521	12.343962	-0.060535	4.815534
297.856562	8000.533298	12.348967	-0.060547	4.815532
298.019995	8000.508218	12.353971	-0.060578	4.815524
297.789814	8000.590982	12.358976	-0.060535	4.815549
297.794891	8000.532276	12.363981	-0.060536	4.815532
297.792805	8000.521553	12.368986	-0.060536	4.815529
297.753070	8000.518757	12.373991	-0.060528	4.815528
297.751744	8000.523011	12.378995	-0.060528	4.815530
297.780477	8000.621828	12.384000	-0.060533	4.815558
297.881535	8000.431100	12.389005	-0.060552	4.815502
297.735273	8000.609321	12.394010	-0.060525	4.815555
297.749029	8000.615963	12.399015	-0.060527	4.815557
297.896639	8000.538243	12.404019	-0.060555	4.815533
297.749483	8000.485564	12.409024	-0.060527	4.815519
297.672762	8000.473603	12.414029	-0.060513	4.815516
297.672577	8000.518495	12.419034	-0.060513	4.815529
297.650559	8000.528819	12.424039	-0.060509	4.815532
297.733894	8000.416898	12.429043	-0.060525	4.815499
297.819062	8000.626748	12.434048	-0.060541	4.815560
298.080396	8000.542364	12.439053	-0.060589	4.815534
297.791444	8000.500159	12.444058	-0.060535	4.815523
297.860180	8000.637052	12.449063	-0.060548	4.815562
298.074400	8000.390480	12.454067	-0.060588	4.815489
298.025987	8000.531843	12.459072	-0.060579	4.815531
298.128992	8000.413833	12.464077	-0.060598	4.815496
298.089770	8000.489076	12.469082	-0.060591	4.815518
297.948074	8000.530552	12.474087	-0.060565	4.815531
297.705250	8000.415358	12.479091	-0.060519	4.815498
297.518721	8000.631391	12.484096	-0.060485	4.815562
297.863851	8000.513122	12.489101	-0.060549	4.815526
297.778639	8000.517054	12.494106	-0.060533	4.815528
297.586113	8000.440107	12.499111	-0.060497	4.815506
297.657127	8000.427389	12.504115	-0.060510	4.815502
297.570703	8000.613015	12.509120	-0.060494	4.815557
297.663805	8000.434983	12.514125	-0.060512	4.815504
297.740182	8000.514281	12.519130	-0.060526	4.815527
297.704987	8000.531869	12.524135	-0.060519	4.815532
298.033284	8000.492420	12.529139	-0.060580	4.815519
297.798537	8000.442564	12.534144	-0.060537	4.815506
297.926496	8000.537682	12.539149	-0.060561	4.815533
297.663052	8000.513004	12.544154	-0.060512	4.815527
297.643811	8000.538339	12.549159	-0.060508	4.815535
297.714541	8000.532030	12.554163	-0.060521	4.815532
297.643692	8000.623851	12.559168	-0.060508	4.815560
297.493186	8000.525153	12.564173	-0.060480	4.815532
297.528786	8000.518261	12.569178	-0.060487	4.815529
297.513310	8000.628103	12.574183	-0.060484	4.815562
297.602580	8000.534451	12.579187	-0.060500	4.815534
297.638442	8000.512599	12.584192	-0.060507	4.815527
297.732865	8000.525924	12.589197	-0.060525	4.815531
297.835873	8000.549011	12.594202	-0.060544	4.815537
297.601568	8000.590019	12.599207	-0.060500	4.815550
297.830440	8000.521130	12.604211	-0.060543	4.815529
297.798277	8000.600766	12.609216	-0.060537	4.815552
297.794039	8000.516251	12.614221	-0.060536	4.815528
297.694314	8000.602249	12.619226	-0.060518	4.815553
297.883457	8000.619283	12.624231	-0.060553	4.815557
297.903410	8000.524480	12.629235	-0.060556	4.815529
297.751527	8000.572201	12.634240	-0.060528	4.815544
297.870029	8000.637233	12.639245	-0.060550	4.815562
297.973535	8000.622917	12.644250	-0.060570	4.815558
297.638053	8000.528632	12.649255	-0.060507	4.815532
297.738375	8000.511056	12.654259	-0.060526	4.815526
297.960634	8000.535053	12.659264	-0.060567	4.815532
297.758794	8000.529567	12.664269	-0.060530	4.815532
297.879818	8000.614951	12.669274	-0.060552	4.815556
297.854698	8000.538641	12.674279	-0.060547	4.815534
297.853787	8000.514042	12.679283	-0.060547	4.815527
297.616547	8000.577449	12.684288	-0.060503	4.815546
297.866681	8000.639320	12.689293	-0.060550	4.815563
297.865601	8000.475758	12.694298	-0.060549	4.815515
297.753511	8000.636374	12.699303	-0.060529	4.815563
297.902038	8000.521258	12.704307	-0.060556	4.815528
297.947590	8000.620354	12.709312	-0.060565	4.815557
297.996539	8000.624374	12.714317	-0.060574	4.815558
297.889609	8000.508226	12.719322	-0.060554	4.815525
298.052986	8000.544073	12.724327	-0.060584	4.815534
298.126463	8000.621186	12.729331	-0.060598	4.815557
297.952294	8000.531714	12.734336	-0.060566	4.815531
297.924187	8000.537662	12.739341	-0.060560	4.815533
298.051821	8000.531228	12.744346	-0.060584	4.815531
297.922261	8000.525873	12.749351	-0.060560	4.815530
297.994113	8000.393451	12.754355	-0.060573	4.815491
297.927614	8000.612545	12.759360	-0.060561	4.815555
297.962570	8000.535094	12.764365	-0.060568	4.815532
297.876587	8000.624527	12.769370	-0.060552	4.815559
297.957713	8000.409952	12.774375	-0.060567	4.815496
298.062432	8000.408482	12.779379	-0.060586	4.815495
297.960334	8000.536128	12.784384	-0.060567	4.815532
298.001233	8000.534669	12.789389	-0.060575	4.815532
298.024674	8000.521162	12.794394	-0.060579	4.815528
297.787565	8000.539677	12.799399	-0.060535	4.815534
297.837042	8000.378024	12.804403	-0.060544	4.815487
297.814456	8000.625637	12.809408	-0.060540	4.815559
297.878741	8000.521950	12.814413	-0.060552	4.815529
298.025202	8000.525449	12.819418	-0.060579	4.815529
297.852497	8000.586720	12.824423	-0.060547	4.815548
297.899129	8000.519083	12.829427	-0.060556	4.815528
297.698539	8000.515757	12.834432	-0.060518	4.815528
297.850079	8000.535373	12.839437	-0.060547	4.815533
297.946040	8000.505967	12.844442	-0.060565	4.815524
298.000599	8000.538940	12.849447	-0.060575	4.815533
297.862342	8000.503510	12.854451	-0.060549	4.815523
297.702941	8000.506212	12.859456	-0.060519	4.815525
298.078197	8000.635363	12.864461	-0.060589	4.815561
297.907801	8000.486094	12.869466	-0.060557	4.815518
298.028492	8000.651642	12.874471	-0.060580	4.815566
298.152038	8000.420667	12.879475	-0.060603	4.815498
298.023201	8000.613073	12.884480	-0.060579	4.815555
298.047742	8000.412524	12.889485	-0.060583	4.815496
297.949413	8000.593679	12.894490	-0.060565	4.815549
297.990847	8000.551610	12.899495	-0.060573	4.815537
298.040279	8000.522500	12.904499	-0.060582	4.815528
297.831774	8000.594935	12.909504	-0.060543	4.815550
297.944464	8000.539083	12.914509	-0.060564	4.815533
297.944432	8000.614977	12.919514	-0.060564	4.815556
298.004272	8000.524043	12.924519	-0.060575	4.815529
298.223669	8000.632437	12.929523	-0.060616	4.815559
297.895998	8000.514765	12.934528	-0.060555	4.815527
297.858771	8000.499183	12.939533	-0.060548	4.815522
297.893615	8000.453799	12.944538	-0.060555	4.815509
297.892262	8000.630148	12.949543	-0.060555	4.815560
297.927810	8000.525984	12.954547	-0.060561	4.815530
297.997238	8000.502551	12.959552	-0.060574	4.815523
298.220246	8000.492355	12.964557	-0.060616	4.815518
298.051881	8000.525905	12.969562	-0.060584	4.815529
297.927954	8000.543091	12.974567	-0.060561	4.815535
298.097551	8000.448633	12.979571	-0.060593	4.815506
298.047113	8000.457417	12.984576	-0.060583	4.815509
297.809252	8000.526158	12.989581	-0.060539	4.815530
297.919105	8000.517292	12.994586	-0.060560	4.815527
298.081726	8000.641847	12.999591	-0.060590	4.815563
298.094670	8000.536239	13.004595	-0.060592	4.815532
297.784390	8000.606985	13.009600	-0.060535	4.815554
298.122005	8000.539900	13.014605	-0.060598	4.815533
298.120286	8000.499253	13.019610	-0.060597	4.815521
297.943235	8000.529453	13.024615	-0.060564	4.815531
298.108641	8000.524715	13.029619	-0.060595	4.815528
297.974197	8000.604792	13.034624	-0.060570	4.815552
298.051259	8000.510937	13.039629	-0.060584	4.815525
297.902490	8000.634602	13.044634	-0.060557	4.815562
298.015749	8000.543485	13.049639	-0.060578	4.815534
297.859427	8000.317491	13.054643	-0.060549	4.815469
297.757109	8000.583021	13.059648	-0.060530	4.815547
298.146197	8000.540306	13.064653	-0.060602	4.815533
298.068668	8000.519780	13.069658	-0.060588	4.815527
297.935666	8000.540021	13.074663	-0.060563	4.815534
298.225891	8000.389843	13.079667	-0.060617	4.815488
298.111732	8000.513013	13.084672	-0.060596	4.815525
297.828310	8000.432419	13.089677	-0.060543	4.815503
298.006309	8000.474922	13.094682	-0.060576	4.815514
298.142561	8000.438701	13.099687	-0.060601	4.815503
297.995764	8000.425578	13.104691	-0.060574	4.815500
297.856946	8000.505582	13.109696	-0.060548	4.815524
298.068113	8000.547566	13.114701	-0.060588	4.815535
298.031327	8000.458237	13.119706	-0.060581	4.815509
298.115036	8000.598585	13.124711	-0.060596	4.815550
298.128945	8000.404273	13.129715	-0.060599	4.815493
298.151754	8000.511543	13.134720	-0.060603	4.815524
297.834606	8000.538351	13.139725	-0.060544	4.815534
297.874746	8000.432126	13.144730	-0.060552	4.815503
298.173860	8000.496947	13.149735	-0.060607	4.815520
297.971769	8000.525662	13.154739	-0.060570	4.815529
297.731135	8000.503500	13.159744	-0.060525	4.815524
297.957893	8000.634463	13.164749	-0.060567	4.815561
298.123013	8000.374249	13.169754	-0.060598	4.815484
297.977478	8000.539655	13.174759	-0.060571	4.815533
298.110197	8000.442448	13.179763	-0.060595	4.815504
297.925284	8000.615752	13.184768	-0.060561	4.815556
297.966355	8000.422960	13.189773	-0.060569	4.815499
298.003879	8000.502683	13.194778	-0.060576	4.815523
298.017705	8000.533911	13.199783	-0.060578	4.815532
298.174866	8000.496968	13.204787	-0.060608	4.815520
297.927885	8000.439426	13.209792	-0.060562	4.815504
298.021720	8000.388607	13.214797	-0.060579	4.815489
298.212495	8000.411012	13.219802	-0.060614	4.815495
297.979979	8000.427465	13.224807	-0.060571	4.815501
298.197347	8000.389383	13.229811	-0.060612	4.815488
298.123362	8000.493979	13.234816	-0.060598	4.815519
298.157563	8000.497753	13.239821	-0.060604	4.815520
298.062029	8000.531444	13.244826	-0.060587	4.815531
298.194554	8000.631984	13.249831	-0.060611	4.815559
298.176671	8000.546173	13.254835	-0.060608	4.815534
297.920398	8000.613540	13.259840	-0.060560	4.815555
298.069355	8000.547601	13.264845	-0.060588	4.815535
298.125366	8000.525014	13.269850	-0.060598	4.815528
298.126499	8000.530378	13.274855	-0.060599	4.815530
298.063827	8000.531477	13.279859	-0.060587	4.815531
298.169047	8000.513982	13.284864	-0.060607	4.815525
298.267733	8000.536998	13.289869	-0.060625	4.815531
298.126362	8000.492965	13.294874	-0.060599	4.815519
298.107589	8000.624132	13.299879	-0.060595	4.815557
298.339665	8000.433438	13.304883	-0.060638	4.815501
297.994229	8000.511084	13.309888	-0.060574	4.815525
298.039581	8000.547111	13.314893	-0.060582	4.815535
298.147436	8000.525385	13.319898	-0.060603	4.815528
298.027090	8000.522320	13.324903	-0.060580	4.815528
297.956238	8000.540386	13.329907	-0.060567	4.815534
298.043038	8000.531137	13.334912	-0.060583	4.815531
298.010159	8000.425838	13.339917	-0.060577	4.815500
298.037590	8000.522496	13.344922	-0.060582	4.815528
298.085139	8000.634453	13.349927	-0.060591	4.815561
298.258853	8000.546477	13.354931	-0.060623	4.815534
298.142971	8000.472937	13.359936	-0.060602	4.815513
297.919665	8000.604986	13.364941	-0.060560	4.815553
298.074756	8000.478220	13.369946	-0.060589	4.815515
298.291125	8000.605805	13.374951	-0.060629	4.815551
298.044290	8000.446717	13.379955	-0.060583	4.815506
297.889050	8000.517898	13.384960	-0.060555	4.815528
297.962553	8000.535151	13.389965	-0.060568	4.815532
298.033092	8000.501048	13.394970	-0.060581	4.815522
298.028746	8000.627109	13.399975	-0.060581	4.815559
298.185989	8000.499309	13.404979	-0.060610	4.815521
298.087761	8000.509438	13.409984	-0.060592	4.815524
298.085783	8000.535060	13.414989	-0.060591	4.815532
298.066321	8000.391503	13.419994	-0.060587	4.815490
297.940852	8000.549759	13.424999	-0.060564	4.815537
298.027255	8000.406890	13.430003	-0.060580	4.815494
298.138789	8000.509218	13.435008	-0.060601	4.815524
297.981760	8000.343070	13.440013	-0.060572	4.815476
298.026660	8000.478498	13.445018	-0.060580	4.815515
298.126742	8000.454505	13.450023	-0.060599	4.815508
298.185245	8000.251314	13.455027	-0.060610	4.815448
298.029466	8000.386620	13.460032	-0.060581	4.815488
297.949389	8000.278402	13.465037	-0.060566	4.815457
298.163033	8000.286221	13.470042	-0.060605	4.815459
298.129848	8000.395768	13.475047	-0.060599	4.815491
298.198329	8000.350941	13.480051	-0.060612	4.815477
297.855745	8000.624246	13.485056	-0.060548	4.815559
297.954000	8000.418507	13.490061	-0.060567	4.815498
297.898435	8000.432551	13.495066	-0.060556	4.815503
298.014332	8000.635430	13.500071	-0.060578	4.815561
298.066706	8000.387241	13.505075	-0.060588	4.815488
298.009371	8000.502802	13.510080	-0.060577	4.815523
298.130473	8000.438539	13.515085	-0.060600	4.815503
298.184842	8000.518541	13.520090	-0.060610	4.815526
298.083631	8000.632306	13.525095	-0.060591	4.815560
298.170472	8000.401792	13.530099	-0.060607	4.815492
297.979642	8000.514070	13.535104	-0.060572	4.815526
298.206606	8000.541351	13.540109	-0.060614	4.815533
298.261157	8000.404366	13.545114	-0.060624	4.815493
298.042289	8000.533282	13.550119	-0.060583	4.815531
298.131312	8000.412902	13.555123	-0.060600	4.815496
298.002011	8000.550786	13.560128	-0.060576	4.815537
297.945903	8000.525271	13.565133	-0.060565	4.815529
298.140843	8000.495369	13.570138	-0.060602	4.815520
298.373035	8000.451119	13.575143	-0.060645	4.815506
298.317055	8000.494017	13.580147	-0.060634	4.815518
298.020506	8000.533993	13.585152	-0.060579	4.815532
298.100835	8000.636873	13.590157	-0.060594	4.815561
298.092470	8000.541601	13.595162	-0.060593	4.815533
297.999803	8000.542202	13.600167	-0.060575	4.815534
298.133191	8000.395836	13.605171	-0.060600	4.815491
297.975396	8000.531109	13.610176	-0.060571	4.815531
298.176286	8000.545131	13.615181	-0.060608	4.815534
298.109805	8000.496996	13.620186	-0.060596	4.815520
297.966080	8000.526680	13.625191	-0.060569	4.815530
298.163745	8000.504305	13.630195	-0.060606	4.815522
298.154702	8000.512707	13.635200	-0.060604	4.815525
298.355855	8000.638971	13.640205	-0.060642	4.815561
298.215985	8000.532965	13.645210	-0.060616	4.815530
298.189012	8000.521829	13.650215	-0.060611	4.815527
298.370116	8000.350600	13.655219	-0.060644	4.815476
298.312774	8000.625431	13.660224	-0.060634	4.815557
298.180348	8000.540927	13.665229	-0.060609	4.815533
298.300923	8000.492689	13.670234	-0.060631	4.815518
298.091575	8000.528766	13.675239	-0.060593	4.815530
298.256805	8000.417133	13.680243	-0.060623	4.815496
298.109693	8000.561135	13.685248	-0.060596	4.815539
298.135743	8000.468572	13.690253	-0.060601	4.815512
298.145666	8000.522183	13.695258	-0.060603	4.815528
298.113641	8000.524859	13.700263	-0.060597	4.815528
298.346204	8000.404722	13.705267	-0.060640	4.815492
298.299520	8000.546115	13.710272	-0.060631	4.815534
298.254175	8000.409610	13.715277	-0.060623	4.815494
298.333431	8000.512473	13.720282	-0.060638	4.815524
298.193987	8000.524056	13.725287	-0.060612	4.815528
298.176984	8000.389091	13.730291	-0.060608	4.815488
298.201477	8000.449357	13.735296	-0.060613	4.815506
298.422307	8000.327957	13.740301	-0.060654	4.815469
298.372779	8000.413718	13.745306	-0.060645	4.815495
298.181687	8000.638230	13.750311	-0.060609	4.815561
298.153699	8000.542631	13.755315	-0.060604	4.815533
298.302758	8000.507692	13.760320	-0.060632	4.815523
298.235812	8000.375105	13.765325	-0.060619	4.815484
298.117072	8000.512095	13.770330	-0.060597	4.815525
298.025535	8000.534093	13.775335	-0.060580	4.815532
298.255946	8000.519745	13.780339	-0.060623	4.815526
298.087761	8000.539402	13.785344	-0.060592	4.815533
298.254181	8000.499407	13.790349	-0.060623	4.815520
298.373685	8000.509941	13.795354	-0.060645	4.815523
298.122213	8000.418119	13.800359	-0.060598	4.815497
298.194713	8000.534765	13.805363	-0.060612	4.815531
298.210078	8000.433473	13.810368	-0.060615	4.815501
298.135809	8000.432241	13.815373	-0.060601	4.815501
298.147697	8000.381131	13.820378	-0.060603	4.815486
298.218281	8000.536227	13.825383	-0.060616	4.815531
298.351187	8000.303270	13.830387	-0.060641	4.815463
298.163744	8000.503255	13.835392	-0.060606	4.815522
298.082110	8000.413181	13.840397	-0.060591	4.815496
298.253828	8000.371136	13.845402	-0.060623	4.815483
298.113274	8000.617863	13.850407	-0.060597	4.815556
298.273975	8000.362919	13.855411	-0.060627	4.815480
298.257990	8000.490925	13.860416	-0.060624	4.815518
298.163234	8000.534248	13.865421	-0.060606	4.815531
298.204373	8000.531724	13.870426	-0.060614	4.815530
298.173871	8000.525874	13.875431	-0.060608	4.815528
298.182283	8000.412709	13.880435	-0.060610	4.815495
297.972067	8000.524665	13.885440	-0.060570	4.815529
298.082481	8000.415330	13.890445	-0.060591	4.815497
298.266692	8000.486797	13.895450	-0.060625	4.815517
298.119910	8000.544222	13.900455	-0.060598	4.815534
298.031371	8000.405932	13.905459	-0.060581	4.815494
298.069168	8000.519865	13.910464	-0.060589	4.815527
298.227567	8000.435910	13.915469	-0.060618	4.815502
298.373452	8000.529189	13.920474	-0.060645	4.815528
298.417462	8000.642158	13.925479	-0.060654	4.815561
298.487293	8000.391050	13.930483	-0.060666	4.815488
298.308922	8000.559119	13.935488	-0.060633	4.815537
298.395081	8000.463277	13.940493	-0.060649	4.815509
298.452144	8000.469568	13.945498	-0.060660	4.815511
298.305182	8000.451097	13.950503	-0.060633	4.815506
298.260983	8000.391574	13.955507	-0.060624	4.815489
298.353135	8000.499995	13.960512	-0.060641	4.815520
298.259944	8000.388351	13.965517	-0.060624	4.815488
298.137701	8000.515662	13.970522	-0.060601	4.815526
298.092151	8000.535217	13.975527	-0.060593	4.815532
298.305941	8000.531281	13.980531	-0.060633	4.815529
298.160076	8000.536345	13.985536	-0.060606	4.815532
298.236992	8000.431798	13.990541	-0.060620	4.815501
298.363308	8000.532235	13.995546	-0.060643	4.815529
298.424196	8000.448800	14.000551	-0.060655	4.815505
298.442270	8000.359311	14.005555	-0.060658	4.815478
298.390751	8000.422592	14.010560	-0.060648	4.815497
298.314330	8000.534631	14.015565	-0.060634	4.815530
298.298550	8000.409305	14.020570	-0.060631	4.815494
298.377225	8000.640430	14.025575	-0.060646	4.815561
298.337375	8000.506153	14.030579	-0.060639	4.815522
298.303707	8000.409392	14.035584	-0.060632	4.815494
298.358808	8000.264934	14.040589	-0.060642	4.815451
298.436087	8000.333558	14.045594	-0.060657	4.815471
298.179862	8000.289759	14.050599	-0.060609	4.815459
298.318199	8000.159510	14.055603	-0.060635	4.815421
298.344148	8000.402583	14.060608	-0.060640	4.815492
298.416771	8000.409133	14.065613	-0.060653	4.815493
298.276433	8000.257158	14.070618	-0.060627	4.815449
298.057457	8000.581683	14.075623	-0.060587	4.815545
298.344049	8000.496648	14.080627	-0.060640	4.815519
298.364761	8000.424306	14.085632	-0.060644	4.815498
298.235539	8000.539744	14.090637	-0.060620	4.815532
298.433435	8000.376275	14.095642	-0.060657	4.815483
298.464451	8000.541405	14.100647	-0.060662	4.815532
298.480991	8000.553438	14.105651	-0.060665	4.815535
298.301650	8000.526946	14.110656	-0.060632	4.815528
298.359465	8000.527906	14.115661	-0.060643	4.815528
298.468749	8000.427103	14.120666	-0.060663	4.815498
298.432132	8000.544078	14.125671	-0.060656	4.815532
298.518636	8000.327453	14.130675	-0.060672	4.815469
298.496895	8000.445743	14.135680	-0.060668	4.815503
298.369181	8000.556931	14.140685	-0.060645	4.815537
298.515713	8000.405437	14.145690	-0.060672	4.815492
298.410430	8000.469964	14.150695	-0.060652	4.815511
298.319070	8000.471656	14.155699	-0.060635	4.815512
298.256589	8000.530479	14.160704	-0.060624	4.815529
298.329078	8000.530613	14.165709	-0.060637	4.815529
298.447538	8000.510132	14.170714	-0.060659	4.815523
298.279338	8000.534065	14.175719	-0.060628	4.815530
298.560152	8000.543000	14.180723	-0.060680	4.815532
298.623045	8000.515183	14.185728	-0.060692	4.815523
298.478617	8000.401619	14.190733	-0.060665	4.815491
298.383286	8000.512275	14.195738	-0.060647	4.815523
298.319761	8000.622390	14.200743	-0.060636	4.815556
298.410625	8000.410113	14.205747	-0.060652	4.815493
298.284938	8000.480715	14.210752	-0.060629	4.815515
298.170360	8000.529054	14.215757	-0.060608	4.815529
298.439571	8000.274842	14.220762	-0.060658	4.815454
298.439638	8000.539936	14.225767	-0.060658	4.815531
298.568689	8000.532457	14.230771	-0.060682	4.815528
298.454197	8000.511317	14.235776	-0.060661	4.815523
298.350213	8000.526695	14.240781	-0.060641	4.815528
298.430774	8000.585754	14.245786	-0.060656	4.815545
298.522192	8000.551997	14.250791	-0.060673	4.815534
298.715493	8000.436553	14.255795	-0.060709	4.815500
298.277494	7999.482253	14.260800	-0.060627	4.815223
298.346961	7996.229053	14.265805	-0.060638	4.814272
298.358489	7990.674286	14.270810	-0.060636	4.812649
298.141966	7983.965451	14.275815	-0.060592	4.810689
298.307795	7976.706240	14.280819	-0.060618	4.808566
298.212280	7968.994754	14.285824	-0.060595	4.806310
298.272298	7961.225381	14.290829	-0.060601	4.804036
298.287397	7953.355592	14.295834	-0.060599	4.801731
298.268986	7945.359102	14.300839	-0.060590	4.799388
298.245080	7937.450569	14.305843	-0.060581	4.797070
298.206788	7929.430719	14.310848	-0.060568	4.794718
298.025266	7921.374429	14.315853	-0.060529	4.792355
298.121505	7913.405957	14.320858	-0.060542	4.790016
297.800493	7905.337618	14.325863	-0.060477	4.787647
297.820517	7897.400361	14.330867	-0.060476	4.785315
298.206095	7889.408355	14.335872	-0.060542	4.782964
298.041532	7881.394562	14.340877	-0.060506	4.780607
297.977826	7873.420093	14.345882	-0.060489	4.778261
298.030786	7865.406605	14.350887	-0.060494	4.775901
297.956587	7857.383741	14.355891	-0.060475	4.773538
297.821805	7849.356691	14.360896	-0.060444	4.771173
297.855488	7841.371816	14.365901	-0.060446	4.768818
297.860232	7833.398982	14.370906	-0.060441	4.766466
297.701396	7825.365679	14.375911	-0.060406	4.764096
297.729896	7817.416935	14.380915	-0.060407	4.761748
297.758857	7809.359077	14.385920	-0.060407	4.759367
297.674277	7801.397886	14.390925	-0.060386	4.757014
297.608302	7793.382846	14.395930	-0.060368	4.754644
297.492936	7785.310095	14.400935	-0.060342	4.752256
297.731009	7777.298123	14.405939	-0.060381	4.749883
297.549717	7769.378195	14.410944	-0.060342	4.747538
297.531764	7761.288129	14.415949	-0.060333	4.745140
297.543549	7753.384602	14.420954	-0.060330	4.742797
297.390783	7745.301243	14.425959	-0.060296	4.740400
297.414352	7737.354248	14.430963	-0.060296	4.738041
297.338682	7729.347146	14.435968	-0.060276	4.735664
297.397552	7721.277138	14.440973	-0.060282	4.733266
297.292118	7713.315677	14.445978	-0.060257	4.730900
297.297113	7705.263784	14.450983	-0.060253	4.728505
297.242785	7697.311935	14.455987	-0.060238	4.726139
297.023862	7689.342686	14.460992	-0.060192	4.723767
297.047520	7681.325189	14.465997	-0.060191	4.721379
297.095567	7673.330812	14.471002	-0.060195	4.718997
297.084373	7665.323210	14.476007	-0.060187	4.716610
297.110989	7657.291738	14.481011	-0.060187	4.714214
297.124904	7649.280977	14.486016	-0.060184	4.711823
297.126270	7641.255371	14.491021	-0.060179	4.709427
297.229455	7633.316133	14.496026	-0.060194	4.707054
297.085974	7625.281902	14.501031	-0.060162	4.704653
297.252081	7617.314634	14.506035	-0.060187	4.702270
297.149530	7609.255553	14.511040	-0.060163	4.699859
296.898656	7601.365405	14.516045	-0.060111	4.697498
296.929470	7593.301986	14.521050	-0.060112	4.695083
297.043585	7585.233883	14.526055	-0.060128	4.692665
296.993121	7577.270879	14.531059	-0.060113	4.690277
296.809957	7569.324667	14.536064	-0.060074	4.687894
296.783385	7561.242075	14.541069	-0.060064	4.685468
296.675015	7553.333679	14.546074	-0.060038	4.683093
296.670463	7545.277208	14.551079	-0.060032	4.680673
296.716712	7537.287487	14.556083	-0.060036	4.678271
296.665150	7529.256728	14.561088	-0.060021	4.675856
296.696252	7521.185957	14.566093	-0.060021	4.673427
296.757368	7513.177578	14.571098	-0.060027	4.671016
296.510167	7505.181227	14.576103	-0.059976	4.668608
296.619295	7497.197925	14.581107	-0.059991	4.666202
296.410393	7489.217368	14.586112	-0.059947	4.663796
296.563093	7481.233159	14.591117	-0.059970	4.661387
296.503277	7473.232568	14.596122	-0.059954	4.658972
296.495932	7465.240482	14.601127	-0.059948	4.656558
296.462222	7457.258658	14.606131	-0.059936	4.654146
296.206483	7449.209036	14.611136	-0.059883	4.651713
296.160181	7441.179849	14.616141	-0.059869	4.649285
296.375276	7433.250514	14.621146	-0.059904	4.646885
296.114804	7425.161068	14.626151	-0.059850	4.644435
296.128416	7417.221941	14.631155	-0.059848	4.642030
296.035557	7409.185777	14.636160	-0.059825	4.639595
296.104737	7401.254045	14.641165	-0.059833	4.637189
296.015096	7393.219132	14.646170	-0.059811	4.634751
296.185861	7385.156031	14.651175	-0.059838	4.632303
296.088465	7377.151194	14.656179	-0.059814	4.629872
296.140320	7369.228855	14.661184	-0.059819	4.627464
296.017117	7361.164675	14.666189	-0.059791	4.625012
295.977495	7353.217755	14.671194	-0.059778	4.622594
296.100795	7345.137733	14.676199	-0.059796	4.620135
295.985297	7337.200202	14.681203	-0.059769	4.617717
296.031501	7329.163479	14.686208	-0.059772	4.615268
296.109777	7321.192443	14.691213	-0.059782	4.612838
296.065819	7313.122247	14.696218	-0.059768	4.610377
295.828026	7305.147452	14.701223	-0.059719	4.607943
295.971449	7297.156361	14.706227	-0.059740	4.605503
296.016733	7289.187909	14.711232	-0.059744	4.603068
295.682775	7281.143314	14.716237	-0.059676	4.600609
295.617891	7273.205954	14.721242	-0.059659	4.598181
295.709955	7265.165534	14.726247	-0.059671	4.595721
295.682895	7257.110192	14.731251	-0.059661	4.593254
295.582983	7249.075615	14.736256	-0.059637	4.590793
295.722937	7241.087731	14.741261	-0.059658	4.588345
295.625860	7233.134051	14.746266	-0.059634	4.585905
295.419452	7225.121821	14.751271	-0.059591	4.583447
295.576516	7217.133447	14.756275	-0.059615	4.580995
295.752110	7209.135026	14.761280	-0.059642	4.578538
295.484583	7201.129875	14.766285	-0.059587	4.576077
295.548518	7193.154553	14.771290	-0.059594	4.573625
295.359795	7185.089941	14.776295	-0.059554	4.571144
295.318207	7177.150969	14.781299	-0.059541	4.568700
295.078548	7169.095366	14.786304	-0.059491	4.566218
295.210632	7161.095522	14.791309	-0.059510	4.563753
295.210768	7153.136917	14.796314	-0.059505	4.561299
294.920089	7145.137263	14.801319	-0.059446	4.558831
295.097393	7137.159255	14.806323	-0.059474	4.556369
295.103765	7129.125633	14.811328	-0.059469	4.553888
295.083815	7121.045005	14.816333	-0.059460	4.551391
295.019031	7113.063942	14.821338	-0.059443	4.548923
295.063023	7105.060456	14.826343	-0.059446	4.546447
295.096033	7097.095665	14.831347	-0.059447	4.543982
295.073890	7089.132470	14.836352	-0.059438	4.541516
295.012520	7081.119445	14.841357	-0.059421	4.539033
295.169128	7073.133721	14.846362	-0.059445	4.536558
294.882767	7065.075495	14.851367	-0.059387	4.534058
294.908227	7057.112405	14.856371	-0.059386	4.531586
294.830937	7049.088988	14.861376	-0.059367	4.529095
294.845326	7041.107589	14.866381	-0.059364	4.526615
294.786810	7033.094921	14.871386	-0.059348	4.524124
294.667907	7025.097156	14.876391	-0.059321	4.521636
294.742777	7017.066345	14.881395	-0.059329	4.519137
294.731785	7009.150848	14.886400	-0.059322	4.516672
294.726147	7001.090378	14.891405	-0.059316	4.514161
294.792655	6992.993794	14.896410	-0.059323	4.511637
294.586651	6985.015974	14.901415	-0.059279	4.509148
294.410187	6977.071409	14.906419	-0.059241	4.506668
294.630960	6969.032008	14.911424	-0.059277	4.504158
294.354840	6961.094177	14.916429	-0.059221	4.501678
294.466389	6953.040621	14.921434	-0.059236	4.499160
294.487943	6945.078161	14.926439	-0.059235	4.496670
294.536887	6937.037084	14.931443	-0.059239	4.494154
294.599367	6929.028282	14.936448	-0.059245	4.491646
294.234828	6921.008088	14.941453	-0.059172	4.489132
294.274652	6913.080198	14.946458	-0.059174	4.486647
294.120734	6904.996420	14.951463	-0.059140	4.484111
294.168989	6897.077343	14.956467	-0.059144	4.481626
294.312868	6889.023499	14.961472	-0.059166	4.479097
294.269769	6881.074468	14.966477	-0.059153	4.476600
294.072395	6873.056093	14.971482	-0.059111	4.474078
294.071423	6865.002477	14.976487	-0.059105	4.471545
294.158780	6856.997080	14.981491	-0.059116	4.469026
294.104881	6849.042368	14.986496	-0.059101	4.466521
294.123050	6841.014054	14.991501	-0.059099	4.463992
294.289316	6833.060835	14.996506	-0.059125	4.461485
294.272512	6824.979632	15.001511	-0.059117	4.458936
293.900824	6817.040849	15.006515	-0.059042	4.456429
293.880280	6809.040118	15.011520	-0.059033	4.453902
293.916296	6800.994837	15.016525	-0.059035	4.451360
293.876532	6793.058763	15.021530	-0.059022	4.448851
293.781402	6784.982861	15.026535	-0.058999	4.446296
293.945698	6776.994056	15.031539	-0.059025	4.443768
293.760711	6769.014360	15.036544	-0.058985	4.441240
293.798362	6761.003797	15.041549	-0.058987	4.438702
293.893350	6753.018685	15.046554	-0.058999	4.436171
293.534774	6744.986318	15.051559	-0.058927	4.433621
293.424499	6736.933613	15.056563	-0.058901	4.431064
293.568665	6728.999920	15.061568	-0.058923	4.428545
293.615929	6720.952265	15.066573	-0.058927	4.425988
293.463852	6712.993628	15.071578	-0.058893	4.423457
293.367534	6704.950501	15.076583	-0.058870	4.420897
293.410085	6697.021769	15.081587	-0.058873	4.418373
293.523246	6688.986742	15.086592	-0.058889	4.415815
293.458163	6680.963969	15.091597	-0.058871	4.413257
293.720610	6672.941766	15.096602	-0.058915	4.410701
293.380403	6664.930672	15.101607	-0.058846	4.408143
293.358610	6656.934939	15.106611	-0.058837	4.405590
293.628376	6648.954786	15.111616	-0.058882	4.403042
293.433140	6640.954520	15.116621	-0.058841	4.400484
293.327529	6633.051197	15.121626	-0.058816	4.397956
293.119460	6624.997154	15.126631	-0.058772	4.395377
293.263386	6616.967321	15.131635	-0.058793	4.392807
293.307838	6608.937020	15.136640	-0.058796	4.390234
293.135402	6600.979425	15.141645	-0.058759	4.387682
292.978892	6592.977606	15.146650	-0.058725	4.385115
293.069658	6584.971309	15.151655	-0.058736	4.382546
292.998470	6576.933699	15.156659	-0.058718	4.379964
293.017218	6569.024538	15.161664	-0.058716	4.377423
293.093842	6560.979126	15.166669	-0.058725	4.374837
293.226735	6552.980098	15.171674	-0.058745	4.372264
292.904482	6544.937015	15.176679	-0.058680	4.369673
293.099342	6536.995688	15.181683	-0.058711	4.367116
292.880686	6528.957377	15.186688	-0.058665	4.364525
292.776349	6520.967229	15.191693	-0.058640	4.361947
293.037400	6512.954443	15.196698	-0.058684	4.359364
292.786765	6505.025952	15.201703	-0.058632	4.356802
292.792412	6496.989912	15.206707	-0.058628	4.354206
292.594227	6488.843983	15.211712	-0.058585	4.351572
292.524420	6480.838474	15.216717	-0.058567	4.348982
292.651812	6472.929224	15.221722	-0.058586	4.346423
292.412717	6464.922255	15.226727	-0.058536	4.343829
292.486473	6456.932938	15.231731	-0.058544	4.341241
292.537584	6448.961354	15.236736	-0.058549	4.338657
292.463555	6440.964443	15.241741	-0.058530	4.336062
292.464860	6432.918825	15.246746	-0.058525	4.333451
292.459595	6424.916644	15.251751	-0.058519	4.330852
292.490994	6416.940569	15.256755	-0.058519	4.328260
292.596073	6408.946534	15.261760	-0.058534	4.325661
292.228333	6400.942795	15.266765	-0.058460	4.323054
292.595403	6392.976523	15.271770	-0.058523	4.320463
292.359663	6384.931702	15.276775	-0.058474	4.317841
292.541922	6376.937910	15.281779	-0.058503	4.315236
292.346842	6368.907765	15.286784	-0.058461	4.312616
292.151900	6360.868240	15.291789	-0.058420	4.309990
292.032296	6352.936118	15.296794	-0.058392	4.307399
292.204593	6344.914094	15.301799	-0.058419	4.304779
292.279447	6336.955521	15.306803	-0.058428	4.302178
292.032717	6328.929283	15.311808	-0.058377	4.299550
291.945238	6320.912806	15.316813	-0.058355	4.296925
292.084230	6312.900540	15.321818	-0.058376	4.294301
291.899161	6304.914379	15.326823	-0.058336	4.291682
291.913793	6296.878767	15.331827	-0.058334	4.289047
291.958931	6288.884430	15.336832	-0.058337	4.286424
291.871941	6280.930599	15.341837	-0.058315	4.283811
291.994522	6272.921283	15.346842	-0.058333	4.281181
291.839692	6264.948582	15.351847	-0.058299	4.278558
291.912774	6256.904796	15.356851	-0.058307	4.275913
291.671234	6248.930028	15.361856	-0.058257	4.273286
291.757544	6240.841828	15.366861	-0.058268	4.270622
291.899034	6232.871782	15.371866	-0.058289	4.267997
291.689512	6224.836361	15.376871	-0.058245	4.265345
291.714135	6216.872629	15.381875	-0.058244	4.262717
291.673377	6208.890982	15.386880	-0.058232	4.260081
291.512554	6200.893922	15.391885	-0.058196	4.257437
291.529505	6192.921617	15.396890	-0.058194	4.254802
291.577699	6184.855282	15.401895	-0.058198	4.252134
291.564759	6176.874880	15.406899	-0.058191	4.249492
291.567356	6168.909388	15.411904	-0.058186	4.246853
291.383723	6160.887198	15.416909	-0.058146	4.244193
291.449564	6152.921448	15.421914	-0.058153	4.241552
291.294547	6144.889778	15.426919	-0.058119	4.238885
291.226157	6136.943473	15.431923	-0.058101	4.236245
291.332652	6128.926685	15.436928	-0.058116	4.233583
291.154460	6120.832083	15.441933	-0.058078	4.230890
291.208337	6112.901066	15.446938	-0.058083	4.228252
291.204808	6104.844477	15.451943	-0.058077	4.225569
291.308792	6096.938812	15.456947	-0.058091	4.222937
291.051205	6088.878363	15.461952	-0.058038	4.220248
290.968684	6080.949872	15.466957	-0.058017	4.217602
291.118248	6072.933383	15.471962	-0.058040	4.214928
290.852959	6064.910187	15.476967	-0.057985	4.212246
291.159868	6056.857042	15.481971	-0.058037	4.209558
291.126054	6048.950038	15.486976	-0.058026	4.206914
290.896094	6040.877785	15.491981	-0.057977	4.204211
290.884941	6032.970890	15.496986	-0.057970	4.201563
290.737614	6024.980087	15.501991	-0.057938	4.198884
290.904067	6016.921283	15.506995	-0.057963	4.196185
290.712911	6008.855655	15.512000	-0.057923	4.193477
290.755608	6000.795321	15.517005	-0.057925	4.190772
290.910297	5992.841592	15.522010	-0.057949	4.188102
290.627187	5984.857764	15.527015	-0.057891	4.185415
290.691007	5976.922696	15.532019	-0.057898	4.182747
290.740481	5968.894837	15.537024	-0.057902	4.180046
290.662226	5960.907854	15.542029	-0.057882	4.177355
290.621894	5952.879422	15.547034	-0.057869	4.174650
290.552953	5944.888639	15.552039	-0.057851	4.171954
290.561330	5936.835727	15.557043	-0.057847	4.169237
290.410334	5928.883081	15.562048	-0.057814	4.166551
290.322079	5920.886404	15.567053	-0.057792	4.163848
290.715655	5912.914611	15.572058	-0.057861	4.161157
290.460258	5904.894324	15.577063	-0.057808	4.158441
290.328892	5896.901868	15.582067	-0.057778	4.155734
290.478026	5888.873671	15.587072	-0.057801	4.153016
290.399782	5880.823582	15.592077	-0.057781	4.150287
290.257614	5872.893318	15.597082	-0.057749	4.147595
290.137403	5864.835081	15.602087	-0.057722	4.144859
290.292292	5856.906677	15.607091	-0.057745	4.142168
290.206433	5848.899162	15.612096	-0.057724	4.139446
290.242858	5840.901770	15.617101	-0.057726	4.136726
290.360893	5832.866348	15.622106	-0.057742	4.133993
290.011908	5824.848464	15.627111	-0.057672	4.131259
289.919951	5816.899075	15.632115	-0.057650	4.128549
289.909414	5808.876010	15.637120	-0.057643	4.125813
289.807787	5800.859790	15.642125	-0.057619	4.123077
289.921442	5792.923274	15.647130	-0.057635	4.120368
289.740589	5784.907845	15.652135	-0.057596	4.117627
289.860594	5776.878416	15.657139	-0.057613	4.114884
289.887516	5768.864170	15.662144	-0.057613	4.112142
289.641265	5760.820873	15.667149	-0.057561	4.109386
289.771828	5752.859024	15.672154	-0.057581	4.106660
289.835385	5744.849425	15.677159	-0.057587	4.103915
289.773577	5736.879070	15.682163	-0.057571	4.101180
289.876378	5728.929566	15.687168	-0.057585	4.098453
289.521828	5720.884849	15.692173	-0.057513	4.095685
289.421447	5712.902150	15.697178	-0.057489	4.092940
289.329093	5704.856489	15.702183	-0.057467	4.090171
289.378032	5696.891488	15.707187	-0.057471	4.087430
289.259426	5688.898542	15.712192	-0.057444	4.084676
289.213675	5680.928989	15.717197	-0.057430	4.081928
289.303380	5672.941345	15.722202	-0.057441	4.079175
289.309955	5664.947011	15.727207	-0.057437	4.076416
289.220940	5656.920362	15.732211	-0.057416	4.073643
289.188926	5648.850868	15.737216	-0.057404	4.070853
289.234264	5640.866816	15.742221	-0.057408	4.068093
289.189421	5632.929721	15.747226	-0.057394	4.065345
288.987909	5624.955761	15.752231	-0.057351	4.062581
289.278490	5616.896842	15.757235	-0.057400	4.059793
289.164906	5608.966239	15.762240	-0.057374	4.057041
289.034184	5600.887089	15.767245	-0.057344	4.054236
289.203261	5592.917034	15.772250	-0.057371	4.051470
288.876609	5584.903064	15.777255	-0.057305	4.048681
288.767833	5576.916110	15.782259	-0.057279	4.045902
288.976970	5568.952648	15.787264	-0.057313	4.043134
288.886596	5560.917650	15.792269	-0.057291	4.040335
288.687044	5552.975323	15.797274	-0.057249	4.037564
288.706370	5544.930705	15.802279	-0.057247	4.034760
288.780065	5536.786482	15.807283	-0.057255	4.031919
288.764937	5528.825210	15.812288	-0.057247	4.029139
288.532485	5520.866381	15.817293	-0.057199	4.026354
288.653881	5512.911112	15.822298	-0.057216	4.023574
288.629752	5504.923971	15.827303	-0.057207	4.020779
288.486157	5496.907550	15.832307	-0.057175	4.017970
288.556040	5488.879350	15.837312	-0.057182	4.015158
288.509729	5480.875261	15.842317	-0.057169	4.012351
288.394029	5472.860328	15.847322	-0.057142	4.009537
288.330968	5464.926046	15.852327	-0.057125	4.006750
288.356632	5456.889410	15.857331	-0.057124	4.003926
288.451653	5448.932523	15.862336	-0.057137	4.001130
288.213679	5440.912015	15.867341	-0.057087	3.998304
288.186085	5432.941764	15.872346	-0.057077	3.995497
288.290237	5424.868366	15.877351	-0.057091	3.992653
288.166505	5416.843016	15.882355	-0.057063	3.989821
288.067392	5408.894808	15.887360	-0.057039	3.987015
288.295701	5400.835438	15.892365	-0.057077	3.984173
288.210586	5392.929671	15.897370	-0.057056	3.981378
287.989573	5384.951124	15.902375	-0.057009	3.978553
288.249469	5376.909041	15.907379	-0.057052	3.975711
288.365191	5368.920817	15.912384	-0.057069	3.972884
288.107259	5360.891626	15.917389	-0.057015	3.970034
287.970223	5352.902174	15.922394	-0.056985	3.967198
287.946927	5344.901643	15.927399	-0.056975	3.964359
287.931829	5336.961830	15.932403	-0.056967	3.961539
287.859435	5328.976873	15.937408	-0.056949	3.958699
287.993316	5320.920159	15.942413	-0.056968	3.955836
288.059726	5312.933878	15.947418	-0.056975	3.952995
287.862467	5304.897803	15.952423	-0.056933	3.950129
287.836629	5296.889921	15.957427	-0.056923	3.947274
287.837769	5288.951273	15.962432	-0.056918	3.944443
287.467294	5280.972805	15.967437	-0.056844	3.941588
287.478968	5272.981389	15.972442	-0.056841	3.938734
287.633441	5264.954634	15.977447	-0.056865	3.935867
287.661837	5256.938205	15.982451	-0.056865	3.933000
287.641482	5248.928311	15.987456	-0.056856	3.930132
287.638835	5240.956493	15.992461	-0.056850	3.927276
287.633584	5232.980168	15.997466	-0.056844	3.924416
287.339019	5225.005166	16.002471	-0.056784	3.921550
287.504425	5216.991037	16.007475	-0.056810	3.918675
287.572415	5209.002457	16.012480	-0.056817	3.915806
287.388073	5200.951036	16.017485	-0.056777	3.912908
287.574231	5192.936071	16.022490	-0.056807	3.910027
287.426445	5184.986625	16.027495	-0.056774	3.907162
287.516773	5176.963207	16.032499	-0.056786	3.904272
287.148041	5169.040505	16.037504	-0.056712	3.901408
287.326709	5160.949969	16.042509	-0.056740	3.898491
287.252638	5152.995296	16.047514	-0.056721	3.895617
287.016977	5144.987672	16.052519	-0.056672	3.892718
286.962681	5136.936870	16.057523	-0.056657	3.889805
287.131712	5128.987217	16.062528	-0.056683	3.886931
287.129000	5120.951705	16.067533	-0.056677	3.884020
287.033333	5113.036508	16.072538	-0.056654	3.881148
287.041168	5105.011571	16.077543	-0.056650	3.878237
286.948582	5097.002354	16.082547	-0.056628	3.875327
286.785212	5088.812334	16.087552	-0.056592	3.872348
286.764228	5080.809808	16.092557	-0.056583	3.869438
286.971966	5072.864369	16.097562	-0.056617	3.866551
286.870545	5064.916768	16.102567	-0.056593	3.863654
286.782383	5056.960752	16.107571	-0.056571	3.860753
286.942031	5048.982621	16.112576	-0.056595	3.857847
286.842826	5040.933201	16.117581	-0.056572	3.854907
286.761661	5032.969286	16.122586	-0.056551	3.851996
286.681809	5024.966965	16.127591	-0.056531	3.849069
286.827602	5016.965046	16.132595	-0.056553	3.846145
286.625051	5009.026107	16.137600	-0.056510	3.843234
286.326443	5000.993887	16.142605	-0.056450	3.840285
286.608217	4993.048552	16.147610	-0.056497	3.837377
286.656121	4985.012602	16.152615	-0.056501	3.834430
286.543914	4977.002927	16.157619	-0.056474	3.831486
286.455203	4969.016809	16.162624	-0.056453	3.828549
286.364569	4960.988609	16.167629	-0.056431	3.825594
286.529665	4953.025800	16.172634	-0.056456	3.822667
286.418354	4945.051841	16.177639	-0.056430	3.819727
286.510453	4937.053743	16.182643	-0.056442	3.816781
286.414572	4929.080258	16.187648	-0.056419	3.813837
286.303517	4921.010738	16.192653	-0.056393	3.810855
286.315702	4913.067953	16.197658	-0.056390	3.807920
286.204147	4905.036397	16.202663	-0.056364	3.804948
286.106574	4897.089619	16.207667	-0.056341	3.802005
286.086012	4889.101548	16.212672	-0.056332	3.799046
286.101648	4881.085591	16.217677	-0.056330	3.796075
285.925239	4873.080529	16.222682	-0.056292	3.793102
285.767773	4865.015137	16.227687	-0.056257	3.790104
285.963895	4857.019998	16.232691	-0.056288	3.787138
285.908879	4849.070374	16.237696	-0.056273	3.784180
285.868722	4841.081657	16.242701	-0.056260	3.781207
286.005128	4833.104564	16.247706	-0.056280	3.778239
285.941331	4825.043599	16.252711	-0.056263	3.775233
285.582475	4817.091429	16.257715	-0.056191	3.772259
285.698957	4809.050819	16.262720	-0.056208	3.769260
285.506584	4801.085477	16.267725	-0.056167	3.766279
285.565297	4793.105360	16.272730	-0.056173	3.763297
285.581397	4785.091626	16.277735	-0.056170	3.760299
285.590729	4777.095532	16.282739	-0.056167	3.757304
285.686566	4769.077170	16.287744	-0.056179	3.754301
285.341316	4761.084967	16.292749	-0.056110	3.751295
285.420898	4753.055526	16.297754	-0.056120	3.748283
285.393649	4745.039156	16.302759	-0.056109	3.745271
285.407475	4737.113839	16.307763	-0.056107	3.742291
285.567965	4729.089455	16.312768	-0.056131	3.739275
285.481221	4721.102746	16.317773	-0.056110	3.736265
285.380519	4713.114289	16.322778	-0.056086	3.733252
285.224054	4705.069671	16.327783	-0.056052	3.730213
285.177568	4697.130522	16.332787	-0.056038	3.727215
285.242355	4689.121335	16.337792	-0.056045	3.724190
285.032814	4681.143548	16.342797	-0.056000	3.721169
285.153662	4673.172654	16.347802	-0.056018	3.718155
284.979943	4665.192462	16.352807	-0.055980	3.715128
284.962403	4657.096846	16.357811	-0.055972	3.712059
285.076202	4649.081723	16.362816	-0.055988	3.709021
285.179915	4641.081173	16.367821	-0.056002	3.705986
285.022666	4633.148424	16.372826	-0.055967	3.702967
284.820770	4625.149633	16.377831	-0.055925	3.699920
284.862329	4617.190002	16.382835	-0.055927	3.696892
284.917663	4609.179455	16.387840	-0.055932	3.693842
284.645193	4601.156930	16.392845	-0.055876	3.690776
284.769779	4593.188646	16.397850	-0.055894	3.687739
284.801918	4585.173332	16.402855	-0.055895	3.684678
284.639698	4577.246133	16.407859	-0.055860	3.681644
284.650741	4569.225109	16.412864	-0.055856	3.678576
284.712022	4561.214764	16.417869	-0.055863	3.675511
284.663455	4553.211094	16.422874	-0.055848	3.672443
284.623545	4545.174499	16.427879	-0.055836	3.669360
284.702286	4537.220451	16.432883	-0.055845	3.666310
284.797194	4529.220724	16.437888	-0.055858	3.663239
284.584794	4521.228967	16.442893	-0.055813	3.660161
284.656198	4513.253173	16.447898	-0.055821	3.657094
284.555773	4505.245488	16.452903	-0.055797	3.654008
284.417582	4497.196996	16.457907	-0.055766	3.650902
284.382032	4489.254376	16.462912	-0.055754	3.647837
284.320294	4481.196581	16.467917	-0.055738	3.644724
284.418850	4473.284891	16.472922	-0.055751	3.641670
284.315411	4465.277536	16.477927	-0.055726	3.638570
284.391197	4457.269498	16.482931	-0.055735	3.635473
284.466518	4449.222374	16.487936	-0.055744	3.632357
284.138565	4441.235930	16.492941	-0.055678	3.629252
284.247082	4433.225228	16.497946	-0.055693	3.626146
284.233807	4425.221026	16.502951	-0.055685	3.623037
284.230580	4417.235045	16.507955	-0.055679	3.619932
284.205125	4409.297588	16.512960	-0.055669	3.616843
283.969126	4401.281603	16.517965	-0.055620	3.613715
283.928942	4393.270833	16.522970	-0.055608	3.610592
283.919520	4385.296038	16.527975	-0.055601	3.607481
283.945451	4377.265670	16.532979	-0.055600	3.604346
283.849854	4369.353169	16.537984	-0.055577	3.601252
283.726536	4361.344173	16.542989	-0.055549	3.598116
283.846462	4353.359862	16.547994	-0.055566	3.594994
283.766144	4345.341074	16.552999	-0.055546	3.591850
283.708092	4337.322968	16.558003	-0.055530	3.588705
283.742600	4329.356921	16.563008	-0.055531	3.585579
283.687769	4321.354232	16.568013	-0.055516	3.582434
283.894521	4313.361030	16.573018	-0.055549	3.579297
283.614049	4305.416580	16.578023	-0.055492	3.576163
283.506872	4297.377036	16.583027	-0.055466	3.572994
283.576441	4289.356278	16.588032	-0.055474	3.569834
283.613378	4281.392448	16.593037	-0.055476	3.566693
283.603447	4273.405882	16.598042	-0.055469	3.563539
283.469450	4265.401604	16.603047	-0.055439	3.560371
283.292639	4257.443970	16.608051	-0.055401	3.557218
283.435128	4249.398068	16.613056	-0.055422	3.554036
283.330668	4241.315477	16.618061	-0.055397	3.550830
283.298652	4233.366215	16.623066	-0.055386	3.547676
283.071319	4225.367121	16.628071	-0.055339	3.544493
283.022921	4217.405097	16.633075	-0.055324	3.541328
283.350716	4209.395269	16.638080	-0.055380	3.538152
283.161594	4201.384408	16.643085	-0.055340	3.534957
282.909832	4193.418506	16.648090	-0.055288	3.531776
283.170494	4185.389792	16.653095	-0.055331	3.528581
283.184450	4177.404948	16.658099	-0.055328	3.525394
283.188878	4169.462416	16.663104	-0.055324	3.522221
282.838895	4161.475278	16.668109	-0.055254	3.519017
283.074586	4153.485073	16.673114	-0.055292	3.515826
282.924211	4145.481783	16.678119	-0.055259	3.512615
282.885039	4137.429086	16.683123	-0.055247	3.509384
282.889552	4129.469869	16.688128	-0.055242	3.506190
282.654392	4121.506138	16.693133	-0.055193	3.502983
282.815918	4113.492691	16.698138	-0.055218	3.499766
282.855766	4105.513052	16.703143	-0.055220	3.496556
282.581166	4097.530356	16.708147	-0.055164	3.493331
282.667211	4089.525461	16.713152	-0.055175	3.490106
282.562058	4081.521244	16.718157	-0.055150	3.486872
282.719337	4073.538680	16.723162	-0.055174	3.483653
282.545084	4065.568663	16.728167	-0.055136	3.480425
282.600148	4057.568001	16.733171	-0.055142	3.477188
282.501331	4049.602334	16.738176	-0.055118	3.473958
282.451093	4041.544848	16.743181	-0.055103	3.470689
282.425712	4033.563743	16.748186	-0.055093	3.467449
282.351166	4025.572520	16.753191	-0.055074	3.464201
282.378602	4017.576090	16.758195	-0.055074	3.460950
282.287569	4009.602009	16.763200	-0.055052	3.457702
282.101240	4001.601748	16.768205	-0.055012	3.454436
282.268493	3993.583781	16.773210	-0.055038	3.451172
282.343846	3985.579969	16.778215	-0.055047	3.447908
282.306509	3977.571421	16.783219	-0.055035	3.444635
282.260591	3969.671929	16.788224	-0.055021	3.441403
282.198497	3961.648545	16.793229	-0.055004	3.438117
282.144968	3953.693100	16.798234	-0.054989	3.434855
281.985854	3945.634389	16.803239	-0.054954	3.431545
281.932929	3937.640987	16.808243	-0.054939	3.428262
281.935760	3929.630959	16.813248	-0.054935	3.424971
281.946767	3921.657552	16.818253	-0.054931	3.421692
282.032879	3913.671204	16.823258	-0.054942	3.418407
281.761745	3905.731059	16.828263	-0.054887	3.415126
281.802768	3897.669976	16.833267	-0.054889	3.411802
281.596666	3889.712796	16.838272	-0.054845	3.408509
281.508308	3881.685669	16.843277	-0.054824	3.405189
281.666517	3873.759030	16.848282	-0.054848	3.401915
281.583033	3865.768943	16.853287	-0.054827	3.398604
281.530142	3857.758532	16.858291	-0.054812	3.395282
281.469136	3849.701016	16.863296	-0.054796	3.391936
281.068674	3841.697297	16.868301	-0.054716	3.388598
281.288420	3833.711705	16.873306	-0.054752	3.385286
281.447234	3825.739726	16.878311	-0.054776	3.381974
281.397266	3817.762441	16.883315	-0.054761	3.378650
281.346219	3809.801360	16.888320	-0.054747	3.375329
281.262279	3801.776922	16.893325	-0.054726	3.371976
281.330836	3793.783364	16.898330	-0.054733	3.368639
281.209436	3785.802731	16.903335	-0.054706	3.365298
281.362927	3777.824446	16.908339	-0.054729	3.361963
281.246616	3769.864496	16.913344	-0.054702	3.358624
280.895115	3761.862070	16.918349	-0.054632	3.355254
281.152308	3753.836206	16.923354	-0.054674	3.351894
280.936000	3745.853232	16.928359	-0.054629	3.348531
280.924679	3737.829488	16.933363	-0.054621	3.345155
281.219213	3729.861414	16.938368	-0.054671	3.341810
280.947912	3721.879323	16.943373	-0.054615	3.338435
280.939099	3713.909922	16.948378	-0.054608	3.335072
280.826699	3705.895565	16.953383	-0.054582	3.331682
280.739162	3697.873224	16.958387	-0.054561	3.328287
280.806820	3689.889733	16.963392	-0.054568	3.324910
280.822297	3681.934378	16.968397	-0.054566	3.321540
280.597907	3673.977329	16.973402	-0.054519	3.318156
280.814507	3665.947674	16.978407	-0.054554	3.314755
280.778084	3657.917717	16.983411	-0.054542	3.311341
280.735577	3649.964078	16.988416	-0.054529	3.307955
280.802326	3641.933430	16.993421	-0.054536	3.304538
280.382674	3634.023190	16.998426	-0.054453	3.301149
280.561455	3625.997661	17.003431	-0.054481	3.297731
280.545148	3617.991252	17.008435	-0.054473	3.294310
280.524881	3610.023442	17.013440	-0.054464	3.290902
280.134163	3602.057826	17.018445	-0.054386	3.287477
280.606807	3594.025875	17.023450	-0.054469	3.284053
280.482859	3586.069732	17.028455	-0.054440	3.280635
280.050615	3578.119306	17.033459	-0.054355	3.277204
280.083675	3570.095330	17.038464	-0.054356	3.273755
280.177712	3562.030030	17.043469	-0.054368	3.270288
280.060158	3554.096073	17.048474	-0.054341	3.266865
280.021428	3546.103972	17.053479	-0.054328	3.263417
280.222450	3538.108547	17.058483	-0.054361	3.259973
280.123298	3530.171353	17.063488	-0.054337	3.256539
280.053831	3522.128788	17.068493	-0.054319	3.253057
280.007968	3514.123681	17.073498	-0.054305	3.249588
280.046059	3506.151796	17.078503	-0.054307	3.246133
279.902283	3498.172110	17.083507	-0.054275	3.242664
280.044253	3490.206907	17.088512	-0.054296	3.239209
280.013863	3482.197255	17.093517	-0.054285	3.235724
279.810095	3474.157186	17.098522	-0.054242	3.232215
279.813935	3466.158155	17.103527	-0.054238	3.228728
279.817571	3458.142758	17.108531	-0.054233	3.225230
279.927819	3450.213944	17.113536	-0.054249	3.221771
279.622240	3442.234814	17.118541	-0.054186	3.218269
279.626170	3434.247572	17.123546	-0.054182	3.214773
279.691242	3426.239062	17.128551	-0.054189	3.211265
279.623283	3418.259640	17.133555	-0.054171	3.207762
279.502714	3410.296075	17.138560	-0.054143	3.204259
279.601584	3402.324762	17.143565	-0.054157	3.200758
279.746472	3394.319483	17.148570	-0.054178	3.197240
279.554724	3386.318131	17.153575	-0.054137	3.193706
279.414980	3378.316536	17.158579	-0.054106	3.190170
279.520208	3370.332292	17.163584	-0.054121	3.186648
279.492074	3362.329358	17.168589	-0.054110	3.183108
279.338484	3354.384022	17.173594	-0.054076	3.179585
279.392644	3346.417060	17.178599	-0.054081	3.176056
279.268830	3338.407828	17.183603	-0.054053	3.172498
279.304935	3330.397146	17.188608	-0.054055	3.168942
279.349632	3322.379173	17.193613	-0.054058	3.165379
279.356253	3314.439085	17.198618	-0.054054	3.161844
279.059026	3306.491134	17.203623	-0.053993	3.158290
278.891323	3298.483742	17.208627	-0.053957	3.154710
279.043920	3290.469004	17.213632	-0.053980	3.151137
278.710908	3282.483454	17.218637	-0.053913	3.147552
278.945305	3274.458666	17.223642	-0.053951	3.143969
279.127002	3266.490541	17.228647	-0.053980	3.140406
278.901571	3258.531696	17.233651	-0.053933	3.136825
278.838285	3250.557077	17.238656	-0.053916	3.133240
278.588772	3242.539896	17.243661	-0.053864	3.129624
278.816959	3234.552858	17.248666	-0.053901	3.126038
278.625075	3226.567977	17.253671	-0.053860	3.122430
278.663929	3218.602739	17.258675	-0.053862	3.118837
278.728289	3210.633080	17.263680	-0.053869	3.115239
278.648543	3202.600712	17.268685	-0.053849	3.111603
278.499199	3194.632257	17.273690	-0.053816	3.107987
278.614268	3186.598565	17.278695	-0.053832	3.104350
278.526000	3178.672946	17.283699	-0.053811	3.100749
278.502889	3170.701988	17.288704	-0.053801	3.097125
278.221152	3162.707379	17.293709	-0.053744	3.093475
278.489402	3154.681370	17.298714	-0.053788	3.089831
278.433331	3146.696038	17.303719	-0.053773	3.086187
278.215590	3138.733090	17.308723	-0.053727	3.082541
278.282555	3130.775421	17.313728	-0.053734	3.078907
278.368447	3122.761796	17.318733	-0.053745	3.075243
278.398255	3114.671456	17.323738	-0.053745	3.071537
278.323113	3106.715810	17.328743	-0.053726	3.067884
278.212943	3098.730459	17.333747	-0.053700	3.064211
277.881920	3090.805132	17.338752	-0.053634	3.060550
278.009258	3082.821511	17.343757	-0.053652	3.056880
278.183118	3074.802031	17.348762	-0.053679	3.053192
278.077378	3066.831036	17.353767	-0.053654	3.049508
277.841579	3058.862868	17.358771	-0.053605	3.045815
277.990191	3050.893824	17.363776	-0.053628	3.042135
277.987903	3042.894040	17.368781	-0.053622	3.038429
277.914645	3034.916752	17.373786	-0.053603	3.034726
277.904136	3026.930636	17.378791	-0.053596	3.031017
277.908841	3018.923864	17.383795	-0.053592	3.027294
277.867386	3010.961908	17.388800	-0.053579	3.023586
277.588663	3002.966886	17.393805	-0.053522	3.019846
277.790780	2995.010547	17.398810	-0.053554	3.016143
277.693923	2987.009043	17.403815	-0.053531	3.012400
277.522546	2979.003345	17.408819	-0.053494	3.008646
277.736179	2971.027877	17.413824	-0.053528	3.004921
277.669716	2963.062411	17.418829	-0.053511	3.001182
277.513193	2955.094482	17.423834	-0.053477	2.997433
277.530287	2947.081093	17.428839	-0.053475	2.993666
277.539309	2939.046161	17.433843	-0.053471	2.989884
277.450147	2931.106607	17.438848	-0.053449	2.986137
277.573264	2923.108890	17.443853	-0.053467	2.982369
277.501501	2915.168376	17.448858	-0.053448	2.978613
277.378463	2907.184035	17.453863	-0.053420	2.974830
277.183198	2899.169559	17.458867	-0.053379	2.971023
277.249096	2891.209855	17.463872	-0.053386	2.967251
277.437123	2883.199847	17.468877	-0.053416	2.963456
277.173145	2875.258399	17.473882	-0.053361	2.959666
276.929051	2867.310053	17.478887	-0.053311	2.955868
276.968921	2859.271417	17.483891	-0.053313	2.952038
277.260546	2851.251296	17.488896	-0.053362	2.948224
277.056406	2843.287208	17.493901	-0.053319	2.944406
276.918890	2835.345240	17.498906	-0.053288	2.940598
276.848835	2827.380920	17.503911	-0.053270	2.936777
276.824752	2819.358289	17.508915	-0.053260	2.932926
276.846615	2811.367174	17.513920	-0.053259	2.929087
276.908889	2803.372387	17.518925	-0.053265	2.925243
276.873527	2795.443434	17.523930	-0.053254	2.921421
276.856625	2787.472410	17.528935	-0.053245	2.917575
276.785115	2779.437167	17.533939	-0.053227	2.913690
276.766966	2771.388110	17.538944	-0.053218	2.909795
276.446012	2763.437937	17.543949	-0.053153	2.905928
276.574335	2755.479834	17.548954	-0.053172	2.902075
276.597349	2747.526523	17.553959	-0.053171	2.898213
276.289950	2739.551091	17.558963	-0.053108	2.894318
276.428161	2731.559566	17.563968	-0.053129	2.890434
276.290722	2723.565823	17.568973	-0.053098	2.886529
276.289116	2715.618334	17.573978	-0.053093	2.882648
276.303086	2707.629403	17.578983	-0.053090	2.878743
276.302867	2699.659899	17.583987	-0.053085	2.874841
276.377460	2691.648302	17.588992	-0.053094	2.870917
276.331116	2683.683410	17.593997	-0.053080	2.867005
276.353140	2675.698897	17.599002	-0.053079	2.863081
276.144730	2667.742356	17.604007	-0.053035	2.859152
275.955978	2659.768068	17.609011	-0.052994	2.855211
275.903235	2651.782597	17.614016	-0.052979	2.851266
275.963117	2643.767707	17.619021	-0.052985	2.847307
275.896897	2635.800266	17.624026	-0.052968	2.843359
275.788665	2627.852467	17.629031	-0.052942	2.839413
275.785574	2619.895032	17.634035	-0.052937	2.835463
275.891136	2611.890508	17.639040	-0.052951	2.831490
275.781393	2603.865298	17.644045	-0.052925	2.827489
275.939176	2595.888552	17.649050	-0.052950	2.823521
275.882977	2587.924906	17.654055	-0.052934	2.819543
275.758291	2579.969767	17.659059	-0.052906	2.815559
275.683145	2572.000329	17.664064	-0.052886	2.811565
275.786327	2563.979442	17.669069	-0.052900	2.807550
275.600904	2556.034893	17.674074	-0.052861	2.803550
275.504130	2548.061773	17.679079	-0.052837	2.799536
275.377152	2540.103011	17.684083	-0.052809	2.795521
275.522921	2532.093252	17.689088	-0.052831	2.791491
275.263356	2524.111071	17.694093	-0.052777	2.787445
275.427763	2516.120392	17.699098	-0.052802	2.783414
275.477068	2508.155816	17.704103	-0.052806	2.779384
275.209056	2500.214508	17.709107	-0.052751	2.775340
275.291746	2492.224957	17.714112	-0.052762	2.771287
275.178921	2484.242299	17.719117	-0.052735	2.767220
275.192151	2476.277503	17.724122	-0.052733	2.763164
275.147015	2468.311669	17.729127	-0.052719	2.759098
275.264416	2460.307981	17.734131	-0.052736	2.755016
275.220820	2452.253936	17.739136	-0.052722	2.750892
274.851668	2444.316714	17.744141	-0.052648	2.746803
274.857133	2436.340005	17.749146	-0.052644	2.742709
275.075162	2428.365851	17.754151	-0.052680	2.738624
274.951409	2420.399095	17.759155	-0.052651	2.734516
274.813918	2412.442377	17.764160	-0.052621	2.730406
274.582639	2404.470187	17.769165	-0.052572	2.726276
274.889562	2396.480551	17.774170	-0.052624	2.722163
274.789216	2388.539910	17.779175	-0.052600	2.718045
274.572059	2380.567559	17.784179	-0.052555	2.713897
274.759457	2372.550135	17.789184	-0.052585	2.709744
274.549015	2364.590143	17.794189	-0.052540	2.705590
274.443549	2356.645468	17.799194	-0.052515	2.701444
274.631858	2348.644869	17.804199	-0.052545	2.697281
274.477050	2340.673334	17.809203	-0.052511	2.693105
274.585642	2332.700974	17.814208	-0.052526	2.688938
274.514479	2324.716194	17.819213	-0.052508	2.684748
274.491699	2316.777875	17.824218	-0.052498	2.680578
274.413532	2308.833119	17.829223	-0.052479	2.676395
274.193869	2300.820865	17.834227	-0.052433	2.672160
274.392986	2292.808393	17.839232	-0.052464	2.667946
274.185977	2284.863203	17.844237	-0.052421	2.663734
274.073876	2276.883171	17.849242	-0.052395	2.659504
274.163362	2268.935425	17.854247	-0.052406	2.655297
274.111337	2260.939380	17.859251	-0.052391	2.651048
274.095479	2252.969642	17.864256	-0.052383	2.646809
273.954387	2245.001392	17.869261	-0.052352	2.642555
274.019644	2237.060169	17.874266	-0.052359	2.638323
273.889534	2229.090594	17.879271	-0.052329	2.634056
273.598162	2221.086564	17.884275	-0.052270	2.629753
273.831133	2213.117490	17.889280	-0.052308	2.625496
273.848894	2205.138426	17.894285	-0.052306	2.621212
273.812292	2197.182022	17.899290	-0.052294	2.616930
274.021069	2189.186515	17.904295	-0.052328	2.612637
273.906017	2181.218809	17.909299	-0.052301	2.608330
273.791706	2173.278665	17.914304	-0.052275	2.604030
273.764637	2165.308275	17.919309	-0.052264	2.599713
273.650120	2157.374702	17.924314	-0.052238	2.595403
273.713686	2149.205295	17.929319	-0.052244	2.590969
273.633758	2141.232311	17.934323	-0.052224	2.586625
273.610607	2133.332605	17.939328	-0.052215	2.582318
273.424550	2125.404265	17.944333	-0.052175	2.577976
273.220689	2117.457975	17.949338	-0.052132	2.573617
273.200004	2109.474868	17.954343	-0.052123	2.569242
273.142504	2101.493810	17.959347	-0.052107	2.564858
273.223642	2093.558565	17.964352	-0.052117	2.560502
273.072147	2085.613519	17.969357	-0.052084	2.556116
273.199367	2077.603619	17.974362	-0.052102	2.551707
273.209932	2069.636963	17.979367	-0.052099	2.547305
272.944781	2061.701354	17.984371	-0.052044	2.542894
273.031402	2053.734051	17.989376	-0.052055	2.538483
273.030861	2045.759359	17.994381	-0.052050	2.534053
272.963449	2037.780796	17.999386	-0.052032	2.529609
272.966991	2029.829601	18.004391	-0.052028	2.525177
272.876826	2021.876984	18.009395	-0.052006	2.520731
272.861101	2013.936431	18.014400	-0.051998	2.516288
272.815553	2005.931351	18.019405	-0.051984	2.511799
272.780849	1997.934208	18.024410	-0.051972	2.507307
272.878852	1989.970923	18.029415	-0.051985	2.502836
272.760160	1982.017646	18.034419	-0.051958	2.498347
272.807442	1974.084367	18.039424	-0.051962	2.493873
272.630198	1966.093386	18.044429	-0.051923	2.489341
272.569884	1958.152842	18.049434	-0.051907	2.484839
272.511315	1950.207529	18.054439	-0.051891	2.480326
272.527010	1942.234683	18.059443	-0.051889	2.475795
272.563111	1934.255142	18.064448	-0.051890	2.471253
272.392689	1926.298304	18.069453	-0.051853	2.466700
272.297228	1918.347016	18.074458	-0.051830	2.462147
272.631883	1910.360512	18.079463	-0.051887	2.457598
272.344704	1902.423795	18.084467	-0.051829	2.453023
272.494981	1894.435741	18.089472	-0.051852	2.448442
272.353414	1886.483530	18.094477	-0.051820	2.443852
272.192074	1878.566782	18.099482	-0.051785	2.439272
272.100003	1870.612441	18.104487	-0.051763	2.434666
272.088335	1862.538202	18.109491	-0.051755	2.429989
272.195736	1854.569660	18.114496	-0.051770	2.425373
271.992414	1846.648735	18.119501	-0.051727	2.420751
272.007391	1838.701552	18.124506	-0.051725	2.416123
272.147658	1830.713947	18.129511	-0.051745	2.411472
272.008928	1822.752322	18.134515	-0.051714	2.406805
271.906973	1814.844976	18.139520	-0.051690	2.402164
271.723139	1806.910218	18.144525	-0.051651	2.397492
271.548927	1798.965894	18.149530	-0.051613	2.392805
271.590648	1790.967632	18.154535	-0.051616	2.388095
271.776032	1782.956647	18.159539	-0.051645	2.383378
271.795135	1775.035594	18.164544	-0.051644	2.378693
271.621229	1767.093690	18.169549	-0.051606	2.373971
271.571610	1759.113974	18.174554	-0.051592	2.369226
271.519381	1751.161096	18.179559	-0.051577	2.364488
271.536582	1743.214824	18.184563	-0.051575	2.359750
271.353594	1735.307859	18.189568	-0.051535	2.355010
271.282907	1727.306698	18.194573	-0.051517	2.350213
271.272970	1719.329539	18.199578	-0.051510	2.345425
271.343937	1711.381037	18.204583	-0.051518	2.340651
271.249511	1703.433359	18.209587	-0.051495	2.335855
271.374049	1695.463510	18.214592	-0.051513	2.331053
271.413367	1687.485507	18.219597	-0.051515	2.326229
271.151207	1679.586205	18.224602	-0.051462	2.321418
271.301527	1671.630960	18.229607	-0.051484	2.316598
271.084791	1663.672931	18.234611	-0.051439	2.311735
271.328219	1655.687697	18.239616	-0.051479	2.306883
271.212305	1647.748965	18.244621	-0.051452	2.302020
271.210006	1639.804861	18.249626	-0.051447	2.297153
271.186506	1631.847736	18.254631	-0.051437	2.292265
271.110332	1623.895070	18.259635	-0.051418	2.287365
271.138686	1615.958222	18.264640	-0.051418	2.282474
270.900327	1608.047672	18.269645	-0.051368	2.277565
270.722845	1600.072134	18.274650	-0.051330	2.272611
270.803276	1592.062060	18.279655	-0.051340	2.267647
270.752734	1584.106418	18.284659	-0.051325	2.262694
270.665119	1576.188621	18.289664	-0.051304	2.257751
270.470511	1568.248425	18.294669	-0.051262	2.252773
270.614399	1560.266822	18.299674	-0.051284	2.247788
270.495701	1552.352586	18.304679	-0.051257	2.242812
270.475198	1544.399880	18.309683	-0.051248	2.237808
270.541245	1536.449894	18.314688	-0.051255	2.232803
270.409503	1528.497723	18.319693	-0.051225	2.227768
270.392368	1520.540895	18.324698	-0.051217	2.222728
270.453268	1512.609093	18.329703	-0.051223	2.217700
270.433703	1504.643040	18.334707	-0.051214	2.212632
270.252293	1496.726823	18.339712	-0.051175	2.207569
270.257803	1488.774717	18.344717	-0.051171	2.202488
270.075726	1480.862059	18.349722	-0.051132	2.197404
269.987755	1472.911537	18.354727	-0.051110	2.192292
269.900861	1464.952557	18.359731	-0.051089	2.187163
270.030975	1456.991694	18.364736	-0.051108	2.182040
270.066901	1449.054580	18.369741	-0.051110	2.176912
269.967717	1441.104075	18.374746	-0.051086	2.171751
269.789392	1433.182344	18.379751	-0.051048	2.166589
269.712700	1425.242854	18.384755	-0.051028	2.161412
269.605554	1417.343967	18.389760	-0.051003	2.156247
269.652830	1409.345254	18.394765	-0.051007	2.151018
269.810064	1401.383014	18.399770	-0.051031	2.145811
269.529373	1393.501274	18.404775	-0.050973	2.140603
269.418636	1385.557985	18.409779	-0.050948	2.135358
269.661678	1377.578274	18.414784	-0.050988	2.130109
269.446976	1369.660560	18.419789	-0.050942	2.124844
269.538957	1361.740984	18.424794	-0.050954	2.119595
269.454424	1353.811114	18.429799	-0.050933	2.114309
269.353679	1345.790142	18.434803	-0.050910	2.108947
269.325793	1337.881165	18.439808	-0.050899	2.103654
269.411510	1329.939849	18.444813	-0.050910	2.098336
269.432480	1321.994343	18.449818	-0.050909	2.092996
269.421373	1314.066797	18.454823	-0.050901	2.087651
269.041023	1306.185298	18.459827	-0.050826	2.082287
269.178564	1298.258200	18.464832	-0.050846	2.076930
268.997583	1290.316611	18.469837	-0.050807	2.071517
268.857053	1282.382438	18.474842	-0.050776	2.066099
268.837313	1274.466350	18.479847	-0.050767	2.060691
268.931079	1266.508663	18.484851	-0.050779	2.055252
268.862831	1258.574108	18.489856	-0.050761	2.049798
268.795269	1250.653353	18.494861	-0.050744	2.044339
268.840683	1242.737640	18.499866	-0.050747	2.038880
268.906513	1234.797264	18.504871	-0.050754	2.033392
268.615190	1226.861880	18.509875	-0.050695	2.027856
268.672462	1218.926315	18.514880	-0.050700	2.022340
268.736868	1211.003680	18.519885	-0.050707	2.016819
268.500702	1203.102761	18.524890	-0.050658	2.011267
268.386658	1195.183745	18.529895	-0.050631	2.005699
268.487548	1187.234096	18.534899	-0.050645	2.000117
268.602259	1179.317518	18.539904	-0.050661	1.994544
268.499588	1171.375052	18.544909	-0.050637	1.988914
268.292324	1163.480580	18.549914	-0.050593	1.983291
268.497464	1155.543685	18.554919	-0.050626	1.977666
268.138956	1147.664113	18.559923	-0.050554	1.972005
268.278300	1139.708447	18.564928	-0.050575	1.966327
268.337867	1131.790808	18.569933	-0.050581	1.960651
268.181769	1123.910990	18.574938	-0.050547	1.954963
268.147275	1115.935994	18.579943	-0.050535	1.949202
268.117003	1108.005036	18.584947	-0.050524	1.943457
268.071462	1100.117636	18.589952	-0.050511	1.937725
267.963355	1092.201577	18.594957	-0.050486	1.931948
267.925927	1084.264036	18.599962	-0.050473	1.926145
267.924793	1076.376206	18.604967	-0.050468	1.920366
267.614114	1068.506901	18.609971	-0.050405	1.914548
267.528151	1060.573831	18.614976	-0.050384	1.908691
267.574462	1052.633943	18.619981	-0.050387	1.902825
267.498799	1044.744740	18.624986	-0.050368	1.896965
267.585084	1036.805912	18.629991	-0.050379	1.891068
267.434563	1028.904566	18.634995	-0.050346	1.885154
267.414575	1021.029262	18.640000	-0.050337	1.879255
267.331084	1013.123599	18.645005	-0.050316	1.873308
267.070817	1005.214829	18.650010	-0.050263	1.867319
267.244409	997.279751	18.655015	-0.050290	1.861342
267.285853	989.360396	18.660019	-0.050292	1.855341
267.346032	981.447736	18.665024	-0.050298	1.849328
267.210729	973.561914	18.670029	-0.050268	1.843294
267.088996	965.684241	18.675034	-0.050240	1.837247
267.022363	957.782312	18.680039	-0.050223	1.831168
266.827021	949.887035	18.685043	-0.050181	1.825059
266.961654	941.989827	18.690048	-0.050201	1.818967
266.696535	934.120169	18.695053	-0.050147	1.812828
266.645850	926.205404	18.700058	-0.050132	1.806659
266.650806	918.321631	18.705063	-0.050128	1.800499
266.561221	910.435509	18.710067	-0.050106	1.794306
266.445995	902.487344	18.715072	-0.050079	1.788038
266.682819	894.555263	18.720077	-0.050118	1.781805
266.598509	886.681531	18.725082	-0.050098	1.775556
266.470917	878.808381	18.730087	-0.050069	1.769280
266.353435	870.935885	18.735091	-0.050042	1.762984
266.461937	863.049497	18.740096	-0.050057	1.756682
266.363180	855.164120	18.745101	-0.050033	1.750332
266.333278	847.276925	18.750106	-0.050023	1.743967
266.412985	839.398642	18.755111	-0.050032	1.737599
266.253195	831.518213	18.760115	-0.049997	1.731176
266.140215	823.661885	18.765120	-0.049971	1.724754
266.270912	815.766495	18.770125	-0.049990	1.718307
265.991689	807.914446	18.775130	-0.049933	1.711819
265.892387	800.027575	18.780135	-0.049910	1.705301
265.790678	792.169776	18.785139	-0.049886	1.698781
266.082140	784.248400	18.790144	-0.049935	1.692235
265.727465	776.411347	18.795149	-0.049864	1.685649
265.735616	768.542932	18.800154	-0.049860	1.679059
265.988398	760.639883	18.805159	-0.049902	1.672446
265.821157	752.769866	18.810163	-0.049866	1.665779
265.464619	744.971288	18.815168	-0.049794	1.659120
265.516340	737.079880	18.820173	-0.049799	1.652410
265.596996	729.184993	18.825178	-0.049809	1.645674
265.598454	721.357606	18.830183	-0.049804	1.638957
265.500734	713.467797	18.835187	-0.049780	1.632145
265.485127	705.583611	18.840192	-0.049772	1.625321
265.380221	697.748213	18.845197	-0.049748	1.618498
265.261645	689.896678	18.850202	-0.049721	1.611630
265.361764	682.032381	18.855207	-0.049734	1.604752
265.077932	674.232146	18.860211	-0.049676	1.597847
265.014141	666.379021	18.865216	-0.049659	1.590896
264.907904	658.534942	18.870221	-0.049634	1.583917
264.979749	650.680003	18.875226	-0.049643	1.576922
264.855343	642.847091	18.880231	-0.049614	1.569888
264.763519	635.009461	18.885235	-0.049592	1.562823
264.882037	627.165516	18.890240	-0.049609	1.555750
264.761987	619.323107	18.895245	-0.049582	1.548612
264.609246	611.502066	18.900250	-0.049548	1.541455
264.744601	603.652995	18.905255	-0.049568	1.534282
264.739154	595.800018	18.910259	-0.049562	1.527051
264.629453	588.002468	18.915264	-0.049537	1.519820
264.695222	580.169082	18.920269	-0.049544	1.512549
264.696202	572.321246	18.925274	-0.049539	1.505219
264.518294	564.557176	18.930279	-0.049501	1.497904
264.305706	556.746347	18.935283	-0.049456	1.490504
264.184661	548.956527	18.940288	-0.049428	1.483101
264.071365	541.160413	18.945293	-0.049402	1.475655
264.062012	533.278334	18.950298	-0.049395	1.468106
264.223795	525.453246	18.955303	-0.049420	1.460601
264.053409	517.673607	18.960307	-0.049383	1.453047
263.807818	509.905758	18.965312	-0.049333	1.445453
263.786458	502.115700	18.970317	-0.049324	1.437834
263.907330	494.280025	18.975322	-0.049341	1.430152
264.001113	486.474747	18.980327	-0.049353	1.422455
263.760466	478.724006	18.985331	-0.049304	1.414714
263.942663	470.904895	18.990336	-0.049332	1.406933
263.687798	463.174619	18.995341	-0.049280	1.399125
263.495302	455.409248	19.000346	-0.049239	1.391248
263.687586	447.590056	19.005351	-0.049270	1.383336
263.533630	439.839123	19.010355	-0.049236	1.375390
263.334265	432.090488	19.015360	-0.049194	1.367393
263.355970	424.324280	19.020365	-0.049193	1.359368
263.333028	416.551949	19.025370	-0.049183	1.351281
263.219460	408.818709	19.030375	-0.049157	1.343170
262.983530	401.090036	19.035379	-0.049108	1.334994
262.959726	393.332164	19.040384	-0.049099	1.326774
263.109322	385.568437	19.045389	-0.049122	1.318527
262.930346	377.757863	19.050394	-0.049083	1.310119
263.071061	369.964079	19.055399	-0.049104	1.301733
262.682761	362.295434	19.060403	-0.049027	1.293331
262.743100	354.561574	19.065408	-0.049033	1.284886
262.871676	346.830611	19.070413	-0.049052	1.276401
262.669829	339.139601	19.075418	-0.049010	1.267842
262.692485	331.430934	19.080423	-0.049009	1.259247
262.516633	323.745850	19.085427	-0.048971	1.250582
262.635874	316.039608	19.090432	-0.048988	1.241889
262.395403	308.388155	19.095437	-0.048938	1.233128
262.125895	300.709750	19.100442	-0.048883	1.224267
261.977594	293.049611	19.105447	-0.048851	1.215386
261.958110	285.352172	19.110451	-0.048842	1.206422
262.027503	277.681444	19.115456	-0.048850	1.197440
261.982211	270.007259	19.120461	-0.048837	1.188363
262.005024	262.343629	19.125466	-0.048836	1.179243
262.016798	254.697489	19.130471	-0.048833	1.170070
261.578258	247.116421	19.135475	-0.048746	1.160811
261.532145	239.467345	19.140480	-0.048733	1.151475
261.670417	231.787634	19.145485	-0.048754	1.142065
261.418748	224.199642	19.150490	-0.048702	1.132607
261.373454	216.585922	19.155495	-0.048688	1.123082
261.376724	208.974238	19.160499	-0.048684	1.113488
261.240336	201.391193	19.165504	-0.048654	1.103817
261.069778	193.832708	19.170509	-0.048617	1.094084
261.123410	186.226172	19.175514	-0.048622	1.084252
260.979694	178.693181	19.180519	-0.048590	1.074381
260.896707	171.115086	19.185523	-0.048570	1.064373
260.837886	163.578920	19.190528	-0.048554	1.054332
260.750968	156.038348	19.195533	-0.048533	1.044182
260.614060	148.536693	19.200538	-0.048503	1.033973
260.727385	140.993685	19.205543	-0.048519	1.023665
260.506639	133.515263	19.210547	-0.048473	1.013261
260.569468	126.013047	19.215552	-0.048480	1.002785
260.387452	118.546954	19.220557	-0.048441	0.992189
260.244834	111.074805	19.225562	-0.048410	0.981480
260.124693	103.640002	19.230567	-0.048382	0.970713
259.955212	96.215645	19.235571	-0.048346	0.959827
259.899238	88.793951	19.240576	-0.048331	0.948850
259.819396	81.387480	19.245581	-0.048311	0.937761
259.651527	74.011507	19.250586	-0.048275	0.926563
259.536297	66.663192	19.255591	-0.048249	0.915284
259.447440	59.519632	19.260595	-0.048228	0.904190