Fri Mar 12 12:18:41 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.800895	0.043317	0.000000	0.000042	0.721122
0.801617	0.043621	0.005005	0.000042	0.721123
0.865801	0.035520	0.010010	0.000030	0.721129
0.673426	0.064456	0.015014	0.000066	0.721119
0.793117	-0.050807	0.020019	0.000044	0.720934
0.833330	-0.087245	0.025024	0.000036	0.720876
1.022456	-0.122079	0.030029	0.000001	0.720874
0.938413	-0.103071	0.035034	0.000017	0.720882
0.673324	-0.060827	0.040038	0.000066	0.720872
0.893887	-0.095388	0.045043	0.000025	0.720882
0.948285	-0.107777	0.050048	0.000015	0.720876
0.784160	-0.078316	0.055053	0.000046	0.720877
0.916108	-0.099080	0.060058	0.000021	0.720882
0.927368	-0.104382	0.065062	0.000019	0.720876
0.683525	-0.058266	0.070067	0.000064	0.720881
0.878324	-0.096133	0.075072	0.000028	0.720875
0.861755	-0.094059	0.080077	0.000031	0.720873
0.790196	-0.179753	0.085082	0.000045	0.720679
0.687850	-0.235636	0.090086	0.000064	0.720533
0.944955	-0.276232	0.095091	0.000016	0.720544
0.881327	-0.266491	0.100096	0.000028	0.720540
0.870247	-0.266227	0.105101	0.000030	0.720537
0.931301	-0.273694	0.110106	0.000018	0.720544
0.865027	-0.300351	0.115110	0.000031	0.720468
0.814991	-0.415463	0.120115	0.000040	0.720224
0.990228	-0.444653	0.125120	0.000007	0.720228
0.996120	-0.449749	0.130125	0.000006	0.720220
1.086318	-0.462170	0.135130	-0.000010	0.720227
0.878860	-0.492314	0.140134	0.000028	0.720095
0.869123	-0.587643	0.145139	0.000030	0.719904
0.825602	-0.581402	0.150144	0.000038	0.719901
0.657089	-0.552188	0.155149	0.000069	0.719899
0.808524	-0.595956	0.160154	0.000041	0.719866
0.664403	-0.706284	0.165158	0.000068	0.719598
0.803859	-0.726927	0.170163	0.000042	0.719606
0.597275	-0.692199	0.175168	0.000081	0.719602
0.651588	-0.754414	0.180173	0.000071	0.719499
0.844193	-0.902875	0.185178	0.000035	0.719274
0.656011	-0.873362	0.190182	0.000070	0.719266
0.627253	-0.863416	0.195187	0.000075	0.719275
0.689798	-1.013444	0.200192	0.000064	0.719001
0.601574	-1.019691	0.205197	0.000080	0.718958
0.708871	-1.034494	0.210202	0.000060	0.718967
0.639985	-1.139424	0.215206	0.000073	0.718735
0.747747	-1.202672	0.220211	0.000053	0.718648
0.620744	-1.182390	0.225216	0.000077	0.718644
0.486825	-1.273391	0.230221	0.000102	0.718417
0.621000	-1.328875	0.235226	0.000077	0.718355
0.361596	-1.284733	0.240230	0.000125	0.718351
0.540875	-1.474931	0.245235	0.000092	0.718038
0.376938	-1.456008	0.250240	0.000122	0.718018
0.417681	-1.505459	0.255245	0.000115	0.717934
0.463187	-1.629015	0.260250	0.000106	0.717706
0.370006	-1.616963	0.265254	0.000124	0.717697
0.442680	-1.743306	0.270259	0.000110	0.717473
0.411225	-1.784603	0.275264	0.000116	0.717380
0.541945	-1.854110	0.280269	0.000092	0.717289
0.497355	-1.945890	0.285274	0.000100	0.717092
0.146230	-1.892149	0.290278	0.000165	0.717074
0.512972	-2.111674	0.295283	0.000097	0.716769
0.247052	-2.071606	0.300288	0.000147	0.716755
0.070595	-2.154488	0.305293	0.000180	0.716528
0.034545	-2.185403	0.310298	0.000186	0.716455
-0.242525	-2.210824	0.315302	0.000238	0.716307
-0.845005	-2.188428	0.320307	0.000350	0.716138
-1.137183	-2.138710	0.325312	0.000404	0.716134
-1.539579	-2.194355	0.330317	0.000479	0.715881
-2.021055	-2.105754	0.335322	0.000569	0.715887
-1.942096	-2.170708	0.340326	0.000554	0.715786
-2.947283	-2.113039	0.345331	0.000741	0.715546
-3.106939	-2.084050	0.350336	0.000771	0.715547
-3.119420	-2.096239	0.355341	0.000773	0.715518
-3.084077	-2.244661	0.360346	0.000767	0.715236
-4.004051	-2.087858	0.365350	0.000938	0.715222
-4.165766	-2.053505	0.370355	0.000968	0.715233
-3.665700	-2.251693	0.375360	0.000875	0.715017
-5.326385	-2.014571	0.380365	0.001184	0.714900
-4.851104	-2.094370	0.385370	0.001096	0.714910
-4.636691	-2.134657	0.390374	0.001056	0.714906
-4.959116	-2.191418	0.395379	0.001116	0.714679
-5.978631	-2.046551	0.400384	0.001306	0.714606
-5.709530	-2.095755	0.405389	0.001256	0.714604
-5.421505	-2.143848	0.410394	0.001202	0.714610
-5.943615	-2.131694	0.415398	0.001299	0.714450
-6.978737	-2.031934	0.420403	0.001492	0.714281
-6.293640	-2.155016	0.425408	0.001365	0.714279
-6.865025	-2.057073	0.430413	0.001471	0.714272
-6.964009	-2.034885	0.435418	0.001489	0.714281
-6.624170	-2.165253	0.440422	0.001426	0.714142
-7.606102	-2.075949	0.445427	0.001609	0.713972
-7.478020	-2.101718	0.450432	0.001585	0.713966
-7.853068	-2.035924	0.455437	0.001655	0.713964
-7.590329	-2.077004	0.460442	0.001606	0.713975
-7.549006	-2.108368	0.465446	0.001598	0.713928
-8.374409	-2.098863	0.470451	0.001752	0.713654
-8.376795	-2.098521	0.475456	0.001752	0.713654
-8.632179	-2.054987	0.480461	0.001800	0.713650
-8.568613	-2.063176	0.485466	0.001788	0.713657
-8.298846	-2.114620	0.490470	0.001738	0.713650
-8.432674	-2.143735	0.495475	0.001763	0.713545
-9.379348	-2.068203	0.500480	0.001939	0.713359
-9.231538	-2.097054	0.505485	0.001911	0.713354
-9.076809	-2.118309	0.510490	0.001883	0.713367
-9.466449	-2.052344	0.515494	0.001955	0.713360
-9.570736	-2.031570	0.520499	0.001975	0.713364
-9.309006	-2.127804	0.525504	0.001926	0.713266
-10.387149	-2.057910	0.530509	0.002127	0.713023
-10.299859	-2.071349	0.535514	0.002110	0.713027
-10.491468	-2.039567	0.540518	0.002146	0.713022
-10.169547	-2.095517	0.545523	0.002086	0.713025
-10.113484	-2.103667	0.550528	0.002076	0.713029
-10.511843	-2.036420	0.555533	0.002150	0.713021
-10.200108	-2.211926	0.560538	0.002092	0.712782
-11.152424	-2.080082	0.565542	0.002269	0.712707
-11.777233	-1.967543	0.570547	0.002385	0.712710
-11.116190	-2.084704	0.575552	0.002262	0.712711
-11.208922	-2.071008	0.580557	0.002280	0.712705
-11.511507	-2.012080	0.585562	0.002336	0.712715
-11.575079	-2.005148	0.590566	0.002348	0.712706
-11.639348	-2.126574	0.595571	0.002360	0.712442
-12.404375	-2.016480	0.600576	0.002502	0.712390
-12.783609	-1.953026	0.605581	0.002573	0.712381
-12.010540	-2.084900	0.610586	0.002429	0.712393
-12.289537	-2.040011	0.615590	0.002481	0.712384
-12.328547	-2.030478	0.620595	0.002488	0.712389
-12.048138	-2.079976	0.625600	0.002436	0.712390
-12.506489	-2.083527	0.630605	0.002521	0.712220
-13.509590	-1.967742	0.635610	0.002708	0.712094
-13.194203	-2.027312	0.640614	0.002649	0.712088
-12.885249	-2.079900	0.645619	0.002592	0.712093
-12.983383	-2.064611	0.650624	0.002610	0.712088
-13.531676	-1.968171	0.655629	0.002712	0.712086
-13.140270	-2.033805	0.660634	0.002639	0.712094
-13.089097	-2.093373	0.665638	0.002630	0.711993
-14.309289	-1.992126	0.670643	0.002857	0.711762
-13.917230	-2.063479	0.675648	0.002784	0.711759
-13.976178	-2.054741	0.680653	0.002795	0.711755
-13.841503	-2.073419	0.685658	0.002770	0.711766
-13.998618	-2.050321	0.690662	0.002799	0.711756
-14.174978	-2.016002	0.695667	0.002832	0.711762
-14.121309	-2.055086	0.700672	0.002822	0.711703
-15.065269	-2.013809	0.705677	0.002997	0.711450
-14.688861	-2.075682	0.710682	0.002927	0.711460
-14.986380	-2.025996	0.715686	0.002983	0.711454
-15.233606	-1.978894	0.720691	0.003029	0.711460
-14.850344	-2.047193	0.725696	0.002957	0.711460
-14.930946	-2.036435	0.730701	0.002972	0.711453
-14.896662	-2.039339	0.735706	0.002966	0.711459
-15.646673	-2.068051	0.740710	0.003106	0.711135
-15.698611	-2.057079	0.745715	0.003115	0.711139
-15.793769	-2.040752	0.750720	0.003133	0.711137
-15.912501	-2.021984	0.755725	0.003155	0.711133
-15.679775	-2.059431	0.760730	0.003112	0.711141
-15.550066	-2.086030	0.765734	0.003088	0.711134
-15.801118	-2.053461	0.770739	0.003134	0.711109
-16.394047	-2.064532	0.775744	0.003245	0.710876
-16.473072	-2.057023	0.780749	0.003260	0.710863
-16.215825	-2.097004	0.785754	0.003212	0.710875
-16.522185	-2.044017	0.790758	0.003269	0.710872
-16.509469	-2.044255	0.795763	0.003266	0.710876
-16.324037	-2.076208	0.800768	0.003232	0.710878
-16.911053	-2.080201	0.805773	0.003341	0.710661
-17.707673	-1.997688	0.810778	0.003489	0.710543
-17.155392	-2.100176	0.815782	0.003387	0.710534
-17.342851	-2.065757	0.820787	0.003421	0.710536
-17.488876	-2.039075	0.825792	0.003449	0.710538
-17.396645	-2.058759	0.830797	0.003431	0.710531
-17.127122	-2.102534	0.835802	0.003381	0.710540
-18.106483	-2.064678	0.840806	0.003564	0.710267
-18.420189	-2.032917	0.845811	0.003622	0.710219
-17.903455	-2.121453	0.850816	0.003526	0.710226
-18.388341	-2.040905	0.855821	0.003616	0.710214
-18.542010	-2.008642	0.860826	0.003645	0.710224
-18.127036	-2.087129	0.865830	0.003567	0.710215
-18.009330	-2.106118	0.870835	0.003546	0.710219
-19.005918	-2.086519	0.875840	0.003731	0.709903
-19.288066	-2.044166	0.880845	0.003784	0.709887
-19.175663	-2.058033	0.885850	0.003763	0.709899
-19.148099	-2.068532	0.890854	0.003758	0.709888
-19.455741	-2.009377	0.895859	0.003815	0.709897
-19.311305	-2.036215	0.900864	0.003788	0.709895
-19.481246	-2.010462	0.905869	0.003820	0.709886
-19.636554	-2.068237	0.910874	0.003848	0.709715
-20.289280	-2.014046	0.915878	0.003970	0.709591
-20.249092	-2.019612	0.920883	0.003962	0.709594
-20.308332	-2.007849	0.925888	0.003974	0.709596
-20.286594	-2.015513	0.930893	0.003969	0.709589
-19.824456	-2.094210	0.935898	0.003883	0.709596
-20.382882	-1.997580	0.940902	0.003987	0.709590
-20.317289	-2.049896	0.945907	0.003975	0.709509
-20.738000	-2.096209	0.950912	0.004054	0.709266
-20.872848	-2.078031	0.955917	0.004079	0.709255
-21.566476	-1.949735	0.960922	0.004208	0.709264
-21.044184	-2.046061	0.965926	0.004111	0.709257
-20.817739	-2.085330	0.970931	0.004068	0.709260
-21.110268	-2.029923	0.975936	0.004123	0.709266
-21.366784	-2.005506	0.980941	0.004171	0.709224
-21.573422	-2.102435	0.985946	0.004209	0.708956
-21.953486	-2.038601	0.990950	0.004280	0.708948
-22.315925	-1.971787	0.995955	0.004347	0.708952
-21.735991	-2.074253	1.000960	0.004239	0.708954
-22.123074	-2.007297	1.005965	0.004311	0.708950
-22.173856	-1.995287	1.010970	0.004321	0.708956
-22.060550	-2.018410	1.015974	0.004300	0.708950
-22.376300	-2.095213	1.020979	0.004359	0.708684
-23.291087	-1.954038	1.025984	0.004529	0.708640
-23.267634	-1.963288	1.030989	0.004524	0.708630
-22.532631	-2.087628	1.035994	0.004388	0.708643
-23.125960	-1.986988	1.040998	0.004498	0.708633
-23.473028	-1.924745	1.046003	0.004563	0.708634
-22.844314	-2.033297	1.051008	0.004446	0.708641
-22.917238	-2.065194	1.056013	0.004459	0.708551
-23.824440	-2.001758	1.061018	0.004628	0.708354
-23.482894	-2.066999	1.066022	0.004565	0.708345
-23.845101	-2.001278	1.071027	0.004632	0.708348
-23.739499	-2.018156	1.076032	0.004612	0.708352
-23.917307	-1.991221	1.081037	0.004645	0.708342
-23.552982	-2.049928	1.086042	0.004578	0.708355
-23.618111	-2.118284	1.091046	0.004590	0.708194
-25.104250	-1.945492	1.096051	0.004866	0.708010
-24.471345	-2.056007	1.101056	0.004749	0.708014
-24.623372	-2.034287	1.106061	0.004777	0.708004
-24.871509	-1.983017	1.111066	0.004823	0.708018
-24.514528	-2.051281	1.116070	0.004757	0.708008
-24.428976	-2.064938	1.121075	0.004741	0.708012
-24.754343	-2.067095	1.126080	0.004801	0.707891
-25.876061	-1.966060	1.131085	0.005010	0.707693
-25.113108	-2.097072	1.136090	0.004868	0.707703
-25.577294	-2.015546	1.141094	0.004954	0.707700
-25.908755	-1.956042	1.146099	0.005016	0.707701
-25.530081	-2.021635	1.151104	0.004946	0.707705
-25.718140	-1.993567	1.156109	0.004981	0.707694
-25.778015	-1.996908	1.161114	0.004992	0.707666
-26.327165	-2.043715	1.166118	0.005094	0.707376
-26.349986	-2.040429	1.171123	0.005098	0.707374
-26.605120	-1.991651	1.176128	0.005146	0.707381
-26.863637	-1.951255	1.181133	0.005194	0.707369
-26.404075	-2.029206	1.186138	0.005108	0.707377
-26.607216	-1.995996	1.191142	0.005146	0.707371
-26.587508	-1.999008	1.196147	0.005142	0.707372
-26.603700	-2.094090	1.201152	0.005146	0.707176
-27.529792	-1.981004	1.206157	0.005318	0.707071
-27.563017	-1.969332	1.211162	0.005324	0.707083
-27.364741	-2.008995	1.216166	0.005287	0.707074
-27.537914	-1.976848	1.221171	0.005319	0.707077
-27.191188	-2.035351	1.226176	0.005255	0.707083
-27.658750	-1.956678	1.231181	0.005342	0.707074
-27.601182	-2.050561	1.236186	0.005331	0.706906
-28.457043	-1.977600	1.241190	0.005491	0.706746
-28.415741	-1.985511	1.246195	0.005483	0.706745
-28.185006	-2.023729	1.251200	0.005440	0.706751
-28.334436	-2.001255	1.256205	0.005468	0.706743
-28.398156	-1.983800	1.261210	0.005480	0.706755
-28.644669	-1.943982	1.266214	0.005525	0.706747
-28.276180	-2.044137	1.271219	0.005457	0.706677
-29.035960	-2.025098	1.276224	0.005598	0.706444
-29.303758	-1.981599	1.281229	0.005648	0.706435
-29.495692	-1.942807	1.286234	0.005684	0.706444
-29.207354	-1.995297	1.291238	0.005630	0.706442
-29.265556	-1.986247	1.296243	0.005641	0.706439
-29.222299	-1.988524	1.301248	0.005633	0.706450
-29.238881	-1.990000	1.306253	0.005636	0.706442
-29.786223	-2.043575	1.311258	0.005738	0.706138
-30.231177	-1.970396	1.316262	0.005821	0.706125
-30.134584	-1.987425	1.321267	0.005803	0.706126
-29.579663	-2.084331	1.326272	0.005700	0.706130
-30.128893	-1.991398	1.331277	0.005802	0.706120
-29.944783	-2.020068	1.336282	0.005767	0.706128
-29.918217	-2.051246	1.341286	0.005763	0.706075
-30.849850	-1.993196	1.346291	0.005936	0.705858
-30.742986	-2.007671	1.351296	0.005916	0.705867
-30.926846	-1.979789	1.356301	0.005950	0.705857
-30.715093	-2.013428	1.361306	0.005911	0.705866
-30.809106	-1.999428	1.366310	0.005928	0.705860
-30.851741	-1.994743	1.371315	0.005936	0.705854
-30.545997	-2.130505	1.376320	0.005879	0.705691
-31.995220	-1.959603	1.381325	0.006149	0.705515
-31.584152	-2.026021	1.386330	0.006073	0.705529
-31.320715	-2.076789	1.391334	0.006024	0.705521
-31.687413	-2.011345	1.396339	0.006092	0.705521
-31.463335	-2.047106	1.401344	0.006050	0.705530
-31.587741	-2.032419	1.406349	0.006073	0.705514
-32.095931	-2.090202	1.411354	0.006168	0.705216
-32.678506	-1.987629	1.416358	0.006276	0.705213
-32.683085	-1.989453	1.421363	0.006277	0.705208
-32.371930	-2.043299	1.426368	0.006219	0.705211
-32.816582	-1.966477	1.431373	0.006302	0.705206
-32.683243	-1.987925	1.436378	0.006277	0.705211
-32.538679	-2.020603	1.441382	0.006250	0.705197
-33.363490	-2.032098	1.446387	0.006404	0.704878
-33.298600	-2.036927	1.451392	0.006392	0.704891
-33.430745	-2.018373	1.456397	0.006416	0.704881
-33.154601	-2.064468	1.461402	0.006365	0.704888
-33.687518	-1.971093	1.466406	0.006464	0.704884
-33.522133	-2.000737	1.471411	0.006433	0.704884
-32.812955	-2.163518	1.476416	0.006301	0.704811
-34.183109	-2.032420	1.481421	0.006557	0.704583
-34.276347	-2.012354	1.486426	0.006574	0.704590
-34.440066	-1.983868	1.491430	0.006604	0.704588
-34.444846	-1.983639	1.496435	0.006605	0.704587
-34.203469	-2.022686	1.501440	0.006560	0.704595
-34.474922	-1.979099	1.506445	0.006611	0.704586
-34.331628	-2.043731	1.511450	0.006584	0.704507
-35.253390	-2.004595	1.516454	0.006756	0.704254
-35.102200	-2.031592	1.521459	0.006728	0.704254
-35.101361	-2.028262	1.526464	0.006727	0.704261
-35.459446	-1.968878	1.531469	0.006794	0.704252
-35.218183	-2.006978	1.536474	0.006749	0.704262
-34.984416	-2.049201	1.541478	0.006706	0.704261
-35.160590	-2.061659	1.546483	0.006738	0.704173
-36.006775	-2.019020	1.551488	0.006896	0.703955
-35.941712	-2.035152	1.556493	0.006884	0.703945
-35.911469	-2.037259	1.561498	0.006878	0.703952
-36.287886	-1.971043	1.566502	0.006948	0.703950
-36.234693	-1.981730	1.571507	0.006938	0.703948
-35.897800	-2.039593	1.576512	0.006876	0.703952
-36.156981	-2.036921	1.581517	0.006924	0.703865
-37.141050	-1.976106	1.586522	0.007107	0.703633
-36.610567	-2.072469	1.591526	0.007008	0.703630
-37.109892	-1.984222	1.596531	0.007101	0.703628
-36.991586	-2.002495	1.601536	0.007079	0.703634
-36.985785	-2.007905	1.606541	0.007078	0.703625
-37.115482	-1.982928	1.611546	0.007102	0.703629
-37.136020	-1.980702	1.616550	0.007106	0.703626
-37.692842	-2.026253	1.621555	0.007210	0.703334
-37.515757	-2.053655	1.626560	0.007177	0.703342
-37.860761	-1.995356	1.631565	0.007241	0.703336
-37.859479	-1.992418	1.636570	0.007241	0.703342
-37.594133	-2.041047	1.641574	0.007192	0.703339
-37.869591	-1.992866	1.646579	0.007243	0.703337
-37.950486	-2.009492	1.651584	0.007258	0.703275
-38.754962	-2.003081	1.656589	0.007408	0.702998
-38.253829	-2.088881	1.661594	0.007314	0.703005
-38.772396	-1.998010	1.666598	0.007411	0.703002
-39.037437	-1.950874	1.671603	0.007460	0.703002
-38.579051	-2.028859	1.676608	0.007375	0.703009
-38.630408	-2.024846	1.681613	0.007384	0.702999
-38.874095	-2.003389	1.686618	0.007430	0.702955
-39.465607	-2.029859	1.691622	0.007540	0.702688
-39.445752	-2.034794	1.696627	0.007536	0.702685
-39.584290	-2.006504	1.701632	0.007562	0.702692
-39.876333	-1.959033	1.706637	0.007616	0.702683
-39.504657	-2.021986	1.711642	0.007547	0.702690
-39.496555	-2.024130	1.716646	0.007546	0.702688
-39.772628	-1.985532	1.721651	0.007597	0.702667
-40.056826	-2.079712	1.726656	0.007650	0.702374
-40.067476	-2.083415	1.731661	0.007652	0.702363
-40.718678	-1.964063	1.736666	0.007773	0.702369
-40.194378	-2.058480	1.741670	0.007676	0.702368
-40.307525	-2.040008	1.746675	0.007697	0.702364
-40.589158	-1.985548	1.751680	0.007749	0.702373
-40.609449	-2.030731	1.756685	0.007753	0.702274
-41.121659	-2.037323	1.761690	0.007848	0.702076
-41.092099	-2.043756	1.766694	0.007843	0.702074
-41.766087	-1.926899	1.771699	0.007968	0.702067
-41.168372	-2.029238	1.776704	0.007857	0.702076
-40.881058	-2.085451	1.781709	0.007803	0.702066
-41.474986	-1.976657	1.786714	0.007914	0.702071
-41.512464	-2.031602	1.791718	0.007921	0.701947
-42.168715	-2.017165	1.796723	0.008043	0.701739
-41.855217	-2.068519	1.801728	0.007985	0.701748
-42.609583	-1.937249	1.806733	0.008125	0.701742
-42.229870	-2.004267	1.811738	0.008055	0.701743
-41.892166	-2.063563	1.816742	0.007992	0.701745
-42.561359	-1.947133	1.821747	0.008116	0.701739
-42.238872	-2.050770	1.826752	0.008056	0.701646
-43.049893	-2.011964	1.831757	0.008207	0.701432
-42.996713	-2.018906	1.836762	0.008197	0.701437
-43.293211	-1.967196	1.841766	0.008252	0.701435
-42.946145	-2.031864	1.846771	0.008188	0.701429
-42.738155	-2.064446	1.851776	0.008149	0.701438
-43.379228	-1.955109	1.856781	0.008268	0.701428
-43.219050	-2.030553	1.861786	0.008239	0.701333
-43.397690	-2.105502	1.866790	0.008272	0.701117
-43.769439	-2.039061	1.871795	0.008341	0.701117
-44.154488	-1.965663	1.876800	0.008413	0.701127
-44.023923	-1.994421	1.881805	0.008389	0.701116
-43.874263	-2.016720	1.886810	0.008361	0.701125
-44.161791	-1.966839	1.891814	0.008414	0.701122
-44.113454	-2.022627	1.896819	0.008405	0.701026
-44.390367	-2.045256	1.901824	0.008457	0.700880
-44.739094	-1.988274	1.906829	0.008522	0.700870
-44.733195	-1.986942	1.911834	0.008521	0.700875
-44.280055	-2.068677	1.916838	0.008436	0.700873
-44.554291	-2.023399	1.921843	0.008487	0.700865
-44.533890	-2.024345	1.926848	0.008483	0.700871
-45.275984	-2.061041	1.931853	0.008622	0.700528
-45.407278	-2.033782	1.936858	0.008646	0.700536
-45.760279	-1.971605	1.941862	0.008712	0.700535
-45.219986	-2.069615	1.946867	0.008611	0.700531
-45.171471	-2.075114	1.951872	0.008602	0.700538
-45.685591	-1.987093	1.956877	0.008698	0.700530
-45.677051	-2.046060	1.961882	0.008696	0.700414
-46.338704	-2.024448	1.966886	0.008819	0.700218
-46.470532	-2.003714	1.971891	0.008844	0.700213
-46.588528	-1.979058	1.976896	0.008866	0.700220
-46.575016	-1.985897	1.981901	0.008863	0.700211
-46.301473	-2.033837	1.986906	0.008813	0.700213
-46.680097	-1.965858	1.991910	0.008883	0.700214
-46.830223	-1.964257	1.996915	0.008911	0.700163
-47.154025	-2.040257	2.001920	0.008971	0.699891
-47.344284	-2.006990	2.011917	0.009007	0.699890
-47.408097	-1.995079	2.021914	0.009019	0.699891
-47.195155	-2.034103	2.031910	0.008979	0.699889
-47.395380	-1.997980	2.041907	0.009016	0.699890
-47.202271	-2.031079	2.051904	0.008980	0.699893
-47.168712	-2.037573	2.061901	0.008974	0.699892
-47.515065	-1.976006	2.071898	0.009038	0.699891
-47.274182	-2.020051	2.081894	0.008994	0.699889
-47.468584	-1.983619	2.091891	0.009030	0.699893
-47.204966	-2.030910	2.101888	0.008981	0.699892
-47.479417	-1.980779	2.111885	0.009032	0.699895
-47.366126	-2.002186	2.121882	0.009011	0.699892
-46.727395	-2.005664	2.131878	0.008892	0.700116
-46.541694	-1.990935	2.141875	0.008857	0.700213
-46.382551	-2.017590	2.151872	0.008827	0.700217
-46.658247	-1.967662	2.161869	0.008879	0.700218
-46.442184	-2.006741	2.171866	0.008839	0.700217
-45.909006	-2.011383	2.181862	0.008739	0.700401
-45.619697	-1.998070	2.191859	0.008685	0.700532
-45.536525	-2.012486	2.201856	0.008670	0.700533
-45.446008	-2.028984	2.211853	0.008653	0.700532
-45.282201	-2.048759	2.221850	0.008623	0.700552
-44.755858	-1.985490	2.231846	0.008524	0.700870
-44.599297	-2.012646	2.241843	0.008495	0.700872
-44.380949	-2.050743	2.251840	0.008455	0.700873
-44.549200	-2.021249	2.261837	0.008486	0.700872
-43.958082	-2.008890	2.271834	0.008376	0.701111
-43.824565	-2.030972	2.281830	0.008351	0.701114
-43.611494	-2.067741	2.291827	0.008311	0.701117
-43.550001	-2.048964	2.301824	0.008300	0.701177
-43.099161	-2.002155	2.311821	0.008216	0.701435
-42.869052	-2.042732	2.321818	0.008173	0.701436
-42.987304	-2.022967	2.331814	0.008195	0.701433
-42.526816	-2.005670	2.341811	0.008109	0.701634
-42.006313	-2.045431	2.351808	0.008012	0.701742
-42.010878	-2.045437	2.361805	0.008013	0.701740
-41.821350	-2.069277	2.371802	0.007978	0.701760
-41.441003	-1.984552	2.381798	0.007907	0.702069
-41.139547	-2.039086	2.391795	0.007851	0.702067
-41.102255	-2.044121	2.401792	0.007844	0.702070
-41.089820	-1.956652	2.411789	0.007842	0.702252
-40.405486	-2.021823	2.421786	0.007714	0.702367
-40.470289	-2.010779	2.431782	0.007726	0.702366
-40.356382	-1.982387	2.441779	0.007705	0.702464
-39.631370	-2.000495	2.451776	0.007570	0.702689
-39.745617	-1.980056	2.461773	0.007591	0.702689
-39.486950	-2.021854	2.471770	0.007543	0.702698
-39.084562	-1.942816	2.481766	0.007468	0.703002
-38.449185	-2.055918	2.491763	0.007350	0.703003
-38.637664	-2.019922	2.501760	0.007385	0.703008
-38.361428	-1.970073	2.511757	0.007334	0.703208
-37.867703	-1.991570	2.521754	0.007242	0.703342
-37.899703	-1.986995	2.531750	0.007248	0.703340
-37.798986	-1.977822	2.541747	0.007229	0.703395
-37.136594	-1.977555	2.551744	0.007105	0.703634
-36.908105	-2.017991	2.561741	0.007063	0.703634
-37.032478	-1.995709	2.571738	0.007086	0.703634
-36.591314	-1.948942	2.581734	0.007004	0.703888
-36.192591	-1.990978	2.591731	0.006930	0.703946
-36.174982	-1.993467	2.601728	0.006926	0.703947
-35.894615	-1.975452	2.611725	0.006874	0.704085
-35.308061	-1.995264	2.621722	0.006765	0.704256
-35.182836	-2.018219	2.631718	0.006742	0.704254
-35.046754	-2.042333	2.641715	0.006716	0.704255
-34.743017	-1.956791	2.651712	0.006660	0.704536
-34.415611	-1.989883	2.661709	0.006599	0.704587
-34.352398	-2.000773	2.671706	0.006587	0.704588
-34.271333	-1.947159	2.681702	0.006572	0.704725
-33.239798	-2.053200	2.691699	0.006380	0.704882
-33.506493	-2.002521	2.701696	0.006429	0.704888
-33.362449	-2.030265	2.711693	0.006403	0.704884
-33.024378	-1.955951	2.721690	0.006340	0.705155
-32.681296	-1.990724	2.731686	0.006276	0.705208
-32.465500	-2.030135	2.741683	0.006236	0.705206
-32.632279	-1.930411	2.751680	0.006267	0.705347
-31.667489	-2.013483	2.761677	0.006087	0.705526
-31.798571	-1.990978	2.771674	0.006111	0.705525
-31.729791	-2.004490	2.781670	0.006099	0.705522
-30.985002	-1.974030	2.791667	0.005960	0.705850
-30.970697	-1.970216	2.801664	0.005957	0.705863
-30.542089	-2.046202	2.811661	0.005877	0.705864
-30.797560	-1.944592	2.821658	0.005925	0.705977
-30.000925	-2.012136	2.831654	0.005777	0.706127
-30.134338	-1.989023	2.841651	0.005801	0.706125
-30.004360	-2.011424	2.851648	0.005777	0.706127
-29.206279	-1.996689	2.861645	0.005629	0.706442
-29.207132	-1.995923	2.871642	0.005629	0.706444
-29.196711	-1.998256	2.881638	0.005627	0.706443
-28.765216	-1.989180	2.891635	0.005546	0.706615
-28.397697	-1.987121	2.901632	0.005478	0.706751
-28.109474	-2.038000	2.911629	0.005424	0.706752
-28.368725	-1.981875	2.921626	0.005473	0.706772
-27.551630	-1.976056	2.931622	0.005320	0.707076
-27.409660	-2.000553	2.941619	0.005294	0.707078
-27.320866	-2.014676	2.951616	0.005277	0.707081
-27.070320	-1.973495	2.961613	0.005231	0.707254
-26.771143	-1.967133	2.971610	0.005175	0.707374
-26.538313	-2.009460	2.981606	0.005132	0.707372
-26.626066	-1.950517	2.991603	0.005148	0.707459
-25.620316	-2.010740	3.001600	0.004961	0.707698
-25.437957	-2.042434	3.011597	0.004927	0.707699
-25.968960	-1.948809	3.021594	0.005026	0.707697
-25.104031	-1.981665	3.031590	0.004865	0.707941
-25.136959	-1.940528	3.041587	0.004871	0.708011
-24.607147	-2.033760	3.051584	0.004772	0.708014
-24.718345	-1.956055	3.061581	0.004793	0.708130
-23.811636	-2.006377	3.071578	0.004624	0.708353
-23.720047	-2.023724	3.081574	0.004607	0.708351
-23.891566	-1.993591	3.091571	0.004639	0.708350
-23.273441	-2.024040	3.101568	0.004524	0.708510
-22.802212	-2.041983	3.111565	0.004436	0.708642
-22.944346	-2.017049	3.121562	0.004462	0.708641
-22.722527	-2.057373	3.131558	0.004421	0.708640
-22.484523	-1.963754	3.141555	0.004377	0.708912
-22.052715	-2.017964	3.151552	0.004296	0.708958
-22.016149	-2.024646	3.161549	0.004290	0.708957
-22.084464	-1.944236	3.171546	0.004302	0.709094
-21.002805	-2.052517	3.181542	0.004101	0.709263
-21.278432	-2.004301	3.191539	0.004152	0.709261
-21.020677	-2.049778	3.201536	0.004104	0.709262
-20.486028	-2.004642	3.211533	0.004005	0.709543
-20.232872	-2.023276	3.221530	0.003957	0.709596
-20.357671	-2.002723	3.231526	0.003981	0.709593
-20.334211	-1.959826	3.241523	0.003976	0.709687
-19.335224	-2.035545	3.251520	0.003790	0.709891
-19.518899	-2.002390	3.261517	0.003824	0.709892
-19.433510	-2.018866	3.271514	0.003809	0.709890
-18.562689	-2.034561	3.281510	0.003646	0.710169
-18.650494	-1.995574	3.291507	0.003663	0.710215
-18.244214	-2.067243	3.301504	0.003587	0.710217
-18.619482	-1.966152	3.311501	0.003657	0.710285
-17.698912	-2.007179	3.321498	0.003486	0.710531
-17.536857	-2.035049	3.331494	0.003455	0.710533
-17.602838	-2.024747	3.341491	0.003468	0.710530
-17.026690	-2.017618	3.351488	0.003360	0.710749
-16.687980	-2.017351	3.361485	0.003297	0.710870
-16.558063	-2.039219	3.371482	0.003273	0.710873
-16.477822	-2.055915	3.381478	0.003258	0.710868
-16.287053	-1.973240	3.391475	0.003223	0.711101
-15.938962	-2.016323	3.401472	0.003158	0.711139
-16.000474	-2.004469	3.411469	0.003169	0.711141
-15.291410	-2.042311	3.421466	0.003037	0.711317
-15.177210	-1.993914	3.431462	0.003016	0.711455
-15.102824	-2.007961	3.441459	0.003002	0.711453
-15.024317	-1.992886	3.451456	0.002987	0.711511
-14.093614	-2.033795	3.461453	0.002814	0.711760
-13.797285	-2.085235	3.471450	0.002759	0.711763
-14.000080	-2.049617	3.481446	0.002797	0.711762
-13.953415	-1.988591	3.491443	0.002788	0.711900
-12.739548	-2.107452	3.501440	0.002562	0.712094
-13.318806	-2.003695	3.511437	0.002670	0.712095
-12.914341	-2.077695	3.521434	0.002595	0.712092
-12.649562	-2.012859	3.531430	0.002545	0.712315
-12.414348	-2.019861	3.541427	0.002501	0.712384
-12.433971	-2.016098	3.551424	0.002505	0.712385
-12.073092	-2.018491	3.561421	0.002438	0.712508
-11.355391	-2.045159	3.571418	0.002304	0.712710
-11.603537	-2.002798	3.581414	0.002350	0.712706
-11.245727	-2.066090	3.591411	0.002284	0.712707
-10.560810	-2.052133	3.601408	0.002156	0.712978
-10.471046	-2.045005	3.611405	0.002139	0.713024
-10.405351	-2.057347	3.621402	0.002127	0.713022
-10.599695	-1.992998	3.631398	0.002163	0.713082
-9.552780	-2.041105	3.641395	0.001968	0.713357
-9.532427	-2.043443	3.651392	0.001965	0.713360
-9.366238	-2.072668	3.661389	0.001934	0.713360
-8.912488	-2.077484	3.671386	0.001849	0.713512
-8.696396	-2.046425	3.681382	0.001809	0.713650
-8.441977	-2.093059	3.691379	0.001762	0.713647
-8.672911	-2.051216	3.701376	0.001805	0.713649
-8.005273	-2.044641	3.711373	0.001680	0.713898
-7.804555	-2.045293	3.721370	0.001643	0.713968
-7.769701	-2.052258	3.731366	0.001636	0.713967
-7.550035	-2.056912	3.741363	0.001595	0.714035
-6.958253	-2.040998	3.751360	0.001485	0.714276
-6.720607	-2.083148	3.761357	0.001441	0.714277
-7.146978	-2.005700	3.771354	0.001520	0.714280
-6.541145	-1.979728	3.781350	0.001408	0.714546
-6.038753	-2.038459	3.791347	0.001314	0.714607
-6.124736	-2.024409	3.801344	0.001330	0.714604
-5.748095	-2.025775	3.811341	0.001260	0.714735
-5.218360	-2.033689	3.821338	0.001161	0.714906
-5.263002	-2.025193	3.831334	0.001170	0.714907
-5.115623	-2.051181	3.841331	0.001142	0.714908
-4.323590	-2.040050	3.851328	0.000995	0.715210
-4.232766	-2.044497	3.861325	0.000978	0.715233
-4.253159	-2.042212	3.871322	0.000981	0.715231
-4.191728	-2.003557	3.881318	0.000970	0.715329
-3.063216	-2.096538	3.891315	0.000760	0.715543
-3.362476	-2.042999	3.901312	0.000816	0.715544
-3.249543	-2.062141	3.911309	0.000795	0.715546
-2.782654	-2.036985	3.921306	0.000708	0.715760
-2.369737	-2.050217	3.931302	0.000631	0.715880
-2.164418	-2.086407	3.941299	0.000593	0.715881
-2.143641	-2.090708	3.951296	0.000589	0.715880
-1.791149	-2.052299	3.961293	0.000523	0.716080
-1.693549	-2.043932	3.971290	0.000505	0.716131
-1.519633	-2.075592	3.981286	0.000472	0.716130
-1.556994	-2.006133	3.991283	0.000479	0.716254
-1.176463	-1.976491	4.001280	0.000408	0.716447
-1.048802	-1.998884	4.011277	0.000385	0.716448
-0.899185	-1.965822	4.021274	0.000357	0.716566
-0.924418	-1.866858	4.031270	0.000361	0.716753
-0.817783	-1.887045	4.041267	0.000342	0.716751
-0.709395	-1.767303	4.051264	0.000321	0.717026
-0.811389	-1.719319	4.061261	0.000340	0.717085
-0.649731	-1.653259	4.071258	0.000310	0.717273
-0.511000	-1.623759	4.081254	0.000284	0.717380
-0.446868	-1.535109	4.091251	0.000272	0.717578
-0.426630	-1.475900	4.101248	0.000268	0.717702
-0.213504	-1.394996	4.111245	0.000229	0.717937
-0.295315	-1.336923	4.121242	0.000244	0.718023
-0.333451	-1.164200	4.131238	0.000251	0.718351
-0.390771	-1.087072	4.141235	0.000261	0.718483
-0.292131	-1.020052	4.151232	0.000243	0.718650
-0.222130	-0.874128	4.161229	0.000230	0.718962
-0.039659	-0.807282	4.171226	0.000196	0.719158
-0.085868	-0.692310	4.181222	0.000204	0.719369
0.146919	-0.614903	4.191219	0.000161	0.719603
0.171684	-0.468762	4.201216	0.000156	0.719900
0.266788	-0.363016	4.211213	0.000138	0.720142
0.029784	-0.188402	4.221210	0.000182	0.720402
-0.052577	-0.026987	4.231206	0.000198	0.720691
0.135713	0.078743	4.241203	0.000163	0.720965
0.000000	0.268595	4.251200	0.000188	0.721291
0.139715	0.878648	4.256205	0.000161	0.722539
0.430418	2.093833	4.261210	0.000106	0.725022
0.536822	3.928859	4.266214	0.000085	0.728640
0.849664	6.278690	4.271219	0.000026	0.733309
1.248253	9.127182	4.276224	-0.000051	0.738934
1.487139	12.475622	4.281229	-0.000097	0.745415
1.685602	16.294753	4.286234	-0.000137	0.752714
2.107022	20.471105	4.291238	-0.000218	0.760683
2.565670	25.042452	4.296243	-0.000306	0.769311
3.099422	29.976884	4.301248	-0.000409	0.778528
3.699822	35.236089	4.306253	-0.000524	0.788243
3.999217	40.882305	4.311258	-0.000583	0.798433
4.453964	46.790893	4.316262	-0.000672	0.809002
5.022259	52.964097	4.321267	-0.000782	0.819928
6.159991	59.324106	4.326272	-0.000998	0.831200
7.991592	65.792126	4.331277	-0.001343	0.842708
8.311250	72.771147	4.336282	-0.001407	0.854467
9.180108	79.845492	4.341286	-0.001574	0.866380
12.321842	86.736404	4.346291	-0.002163	0.878480
12.835470	94.293371	4.351296	-0.002264	0.890739
13.463641	101.968218	4.356301	-0.002386	0.903048
14.592894	109.722693	4.361306	-0.002601	0.915451
15.301637	117.649494	4.366310	-0.002738	0.927838
16.093925	125.688078	4.371315	-0.002891	0.940252
17.181801	133.794494	4.376320	-0.003099	0.952682
18.148349	141.996171	4.381325	-0.003284	0.965059
19.053385	150.310899	4.386330	-0.003458	0.977428
19.955544	158.696872	4.391334	-0.003631	0.989743
20.594306	167.162324	4.396339	-0.003756	1.001954
21.487711	175.620752	4.401344	-0.003928	1.014069
21.895719	184.190621	4.406349	-0.004009	1.026079
22.901039	192.710059	4.411354	-0.004202	1.038022
23.961644	201.240680	4.416358	-0.004405	1.049856
24.689766	209.861176	4.421363	-0.004546	1.061601
25.426397	218.519742	4.426368	-0.004689	1.073269
26.052244	227.169129	4.431373	-0.004811	1.084775
26.695114	235.841882	4.436378	-0.004937	1.096193
27.479862	244.476861	4.441382	-0.005088	1.107476
28.397323	253.092460	4.446387	-0.005265	1.118650
29.159769	261.754835	4.451392	-0.005412	1.129737
29.771735	270.425676	4.456397	-0.005532	1.140695
30.635344	279.079185	4.461402	-0.005698	1.151580
31.716030	287.665991	4.466406	-0.005905	1.162326
32.345400	296.314747	4.471411	-0.006028	1.172956
32.929494	304.959191	4.476416	-0.006143	1.183475
33.785211	313.543635	4.481421	-0.006307	1.193884
34.571128	322.121555	4.486426	-0.006459	1.204182
35.238405	330.717490	4.491430	-0.006589	1.214389
36.024360	339.268629	4.496435	-0.006741	1.224483
36.857293	347.845751	4.501440	-0.006902	1.234532
37.603827	356.369445	4.506445	-0.007046	1.244423
38.720986	364.858428	4.511450	-0.007260	1.254266
39.153742	373.424590	4.516454	-0.007346	1.263990
39.581830	381.990193	4.521459	-0.007431	1.273637
40.278861	390.481358	4.526464	-0.007567	1.283180
41.143988	398.932469	4.531469	-0.007733	1.292639
41.946999	407.391551	4.536474	-0.007888	1.302026
42.441826	415.970753	4.541478	-0.007986	1.311419
43.509911	424.391707	4.546483	-0.008191	1.320679
44.358824	432.802646	4.551488	-0.008354	1.329824
44.699962	441.272936	4.556493	-0.008423	1.338879
45.387130	449.676097	4.561498	-0.008557	1.347863
45.971962	458.095820	4.566502	-0.008671	1.356787
46.369530	466.500143	4.571507	-0.008750	1.365604
46.918335	474.901629	4.576512	-0.008858	1.374387
47.339443	483.287749	4.581517	-0.008942	1.383077
47.838717	491.681558	4.586522	-0.009040	1.391733
48.337747	500.036557	4.591526	-0.009139	1.400297
49.275244	508.309595	4.596531	-0.009319	1.408798
50.129971	516.628371	4.601536	-0.009483	1.417281
50.929163	524.916356	4.606541	-0.009638	1.425673
51.481633	533.284039	4.611546	-0.009746	1.434053
52.074916	541.603901	4.616550	-0.009862	1.442345
52.502466	549.940365	4.621555	-0.009947	1.450578
53.101034	558.255923	4.626560	-0.010064	1.458772
53.696680	566.545575	4.631565	-0.010180	1.466895
54.314207	574.899757	4.636570	-0.010300	1.475037
54.623637	583.208632	4.641574	-0.010363	1.483044
55.537690	591.423727	4.646579	-0.010539	1.491012
56.389376	599.671916	4.651584	-0.010703	1.498959
56.915112	607.943676	4.656589	-0.010806	1.506836
57.613986	616.220062	4.661594	-0.010942	1.514703
57.996809	624.511506	4.666598	-0.011018	1.522494
58.318534	632.805149	4.671603	-0.011084	1.530239
59.234960	641.018608	4.676608	-0.011260	1.537960
59.783000	649.249106	4.681613	-0.011367	1.545602
60.375509	657.528253	4.686618	-0.011483	1.553258
60.811203	665.777205	4.691622	-0.011569	1.560826
61.276787	674.018906	4.696627	-0.011662	1.568354
61.731596	682.282765	4.701632	-0.011752	1.575865
61.950917	690.536302	4.706637	-0.011798	1.583297
62.510638	698.760465	4.711642	-0.011907	1.590717
63.188606	706.960160	4.716646	-0.012039	1.598097
63.591929	715.167493	4.721651	-0.012119	1.605411
64.416595	723.362441	4.726656	-0.012278	1.612740
64.656915	731.609259	4.731661	-0.012328	1.619999
65.214075	739.811856	4.736666	-0.012438	1.627232
65.487202	748.114662	4.741670	-0.012494	1.634479
66.113928	756.260362	4.746675	-0.012616	1.641608
66.892467	764.411652	4.751680	-0.012766	1.648731
67.131132	772.643049	4.756685	-0.012816	1.655818
67.774955	780.806751	4.761690	-0.012941	1.662872
68.264310	789.008482	4.766694	-0.013038	1.669908
68.431073	797.243847	4.771699	-0.013074	1.676899
68.879697	805.424800	4.776704	-0.013163	1.683853
69.388977	813.588932	4.781709	-0.013263	1.690772
69.925016	821.779865	4.786714	-0.013368	1.697688
70.319698	829.960964	4.791718	-0.013447	1.704550
70.954925	838.129274	4.796723	-0.013571	1.711405
71.543051	846.303781	4.801728	-0.013685	1.718231
71.982606	854.441417	4.806733	-0.013773	1.724980
72.482915	862.616004	4.811738	-0.013871	1.731741
73.251279	870.743874	4.816742	-0.014019	1.738472
73.802287	878.891146	4.821747	-0.014127	1.745165
74.203337	887.093930	4.826752	-0.014207	1.751857
74.389319	895.294836	4.831757	-0.014247	1.758496
75.117970	903.395401	4.836762	-0.014388	1.765097
75.719731	911.559314	4.841766	-0.014506	1.771708
76.188316	919.718601	4.846771	-0.014598	1.778274
76.790534	927.871438	4.851776	-0.014716	1.784827
77.394785	936.042694	4.856781	-0.014834	1.791371
77.765975	944.239931	4.861786	-0.014908	1.797883
78.327659	952.349453	4.866790	-0.015018	1.804325
78.597750	960.520629	4.871795	-0.015074	1.810757
78.724753	968.723205	4.876800	-0.015103	1.817174
79.064063	976.852413	4.881805	-0.015171	1.823536
79.378885	985.005457	4.886810	-0.015235	1.829892
79.960853	993.116927	4.891814	-0.015349	1.836225
80.090278	1001.276911	4.896819	-0.015378	1.842521
80.660839	1009.404617	4.901824	-0.015490	1.848821
81.333283	1017.501218	4.906829	-0.015620	1.855089
81.630806	1025.652837	4.911834	-0.015681	1.861333
82.032040	1033.803306	4.916838	-0.015761	1.867568
82.253327	1042.007009	4.921843	-0.015807	1.873801
82.681231	1050.104760	4.926848	-0.015892	1.879957
83.317554	1058.169659	4.931853	-0.016016	1.886092
84.016711	1066.283582	4.936858	-0.016152	1.892251
84.212044	1074.451258	4.941862	-0.016193	1.898373
84.555868	1082.559343	4.946867	-0.016263	1.904447
85.242792	1090.665708	4.951872	-0.016396	1.910540
85.533175	1098.813950	4.956877	-0.016455	1.916599
85.722317	1106.953930	4.961882	-0.016496	1.922622
86.033051	1115.090436	4.966886	-0.016559	1.928637
86.524894	1123.197189	4.971891	-0.016656	1.934631
86.975194	1131.312882	4.976896	-0.016745	1.940609
87.472659	1139.411285	4.981901	-0.016843	1.946560
88.101378	1147.541502	4.986906	-0.016965	1.952531
88.610294	1155.659822	4.991910	-0.017065	1.958462
88.979043	1163.742499	4.996915	-0.017139	1.964333
89.608250	1171.836412	5.001920	-0.017262	1.970224
90.272882	1179.921041	5.006925	-0.017391	1.976093
90.791911	1188.026197	5.011930	-0.017492	1.981945
91.279592	1196.139379	5.016934	-0.017589	1.987781
91.633732	1204.279315	5.021939	-0.017660	1.993605
91.837350	1212.422490	5.026944	-0.017703	1.999398
92.317438	1220.498935	5.031949	-0.017798	2.005157
92.980131	1228.578184	5.036954	-0.017926	2.010919
93.800457	1236.661869	5.041958	-0.018084	2.016685
93.945510	1244.797266	5.046963	-0.018117	2.022400
94.561578	1252.900667	5.051968	-0.018237	2.028125
95.043388	1261.036942	5.056973	-0.018332	2.033844
95.236608	1269.171924	5.061978	-0.018373	2.039515
95.610529	1277.259187	5.066982	-0.018448	2.045156
95.969014	1285.360729	5.071987	-0.018520	2.050790
96.579103	1293.461835	5.076992	-0.018639	2.056433
96.831721	1301.561333	5.081997	-0.018691	2.062024
97.213524	1309.664386	5.087002	-0.018768	2.067615
97.741098	1317.766595	5.092006	-0.018871	2.073205
97.864848	1325.877013	5.097011	-0.018899	2.078745
98.104899	1333.978003	5.102016	-0.018949	2.084275
98.475955	1342.060235	5.107021	-0.019024	2.089791
98.674155	1350.200077	5.112026	-0.019066	2.095314
98.845837	1358.311870	5.117030	-0.019103	2.100801
99.561930	1366.330909	5.122035	-0.019242	2.106264
100.217364	1374.450003	5.127040	-0.019369	2.111775
100.241675	1382.602492	5.132045	-0.019379	2.117232
100.532861	1390.674818	5.137050	-0.019438	2.122647
100.875506	1398.745329	5.142054	-0.019507	2.128052
101.139650	1406.841563	5.147059	-0.019562	2.133453
101.729971	1414.890706	5.152064	-0.019677	2.138840
102.154725	1422.951215	5.157069	-0.019761	2.144205
102.474042	1431.054933	5.162074	-0.019826	2.149575
102.867566	1439.175697	5.167078	-0.019905	2.154950
103.041034	1447.243103	5.172083	-0.019942	2.160256
103.514637	1455.312073	5.177088	-0.020036	2.165578
103.723803	1463.414233	5.182093	-0.020080	2.170883
104.127534	1471.500320	5.187098	-0.020160	2.176184
104.630945	1479.563638	5.192102	-0.020259	2.181465
104.786595	1487.663613	5.197107	-0.020294	2.186726
105.225250	1495.764198	5.202112	-0.020381	2.192000
105.664461	1503.837030	5.207117	-0.020468	2.197244
106.139264	1511.879493	5.212122	-0.020561	2.202458
106.637220	1519.955654	5.217126	-0.020659	2.207684
107.058504	1528.019388	5.222131	-0.020743	2.212883
107.496925	1536.123494	5.227136	-0.020830	2.218096
108.009693	1544.168598	5.232141	-0.020931	2.223267
108.299305	1552.288202	5.237146	-0.020990	2.228452
108.714622	1560.393073	5.242150	-0.021073	2.233628
108.808898	1568.486830	5.247155	-0.021095	2.238756
109.144640	1576.557588	5.252160	-0.021163	2.243878
109.378757	1584.636143	5.257165	-0.021212	2.248986
109.647803	1592.729623	5.262170	-0.021267	2.254094
110.030971	1600.798373	5.267174	-0.021344	2.259184
110.532990	1608.817629	5.272179	-0.021443	2.264243
111.116157	1616.900789	5.277184	-0.021557	2.269337
111.425030	1625.071384	5.282189	-0.021619	2.274450
111.788427	1633.098335	5.287194	-0.021692	2.279467
112.213845	1641.142995	5.292198	-0.021777	2.284490
112.314700	1649.230192	5.297203	-0.021801	2.289500
112.725905	1657.316019	5.302208	-0.021883	2.294524
112.963498	1665.376472	5.307213	-0.021932	2.299507
113.388481	1673.425559	5.312218	-0.022017	2.304488
113.547871	1681.531319	5.317222	-0.022052	2.309471
113.733467	1689.623274	5.322227	-0.022091	2.314436
114.161760	1697.651192	5.327232	-0.022176	2.319372
114.415548	1705.712380	5.332237	-0.022229	2.324303
114.839286	1713.780309	5.337242	-0.022313	2.329242
115.526450	1721.831106	5.342246	-0.022446	2.334182
115.792113	1729.893712	5.347251	-0.022501	2.339083
116.202887	1737.968223	5.352256	-0.022583	2.343994
116.832883	1746.002768	5.357261	-0.022705	2.348887
117.245199	1754.108122	5.362266	-0.022787	2.353796
117.362037	1762.213584	5.367270	-0.022814	2.358670
117.730851	1770.236684	5.372275	-0.022888	2.363505
117.959327	1778.340081	5.377280	-0.022936	2.368366
118.308707	1786.406307	5.382285	-0.023006	2.373206
118.498838	1794.484642	5.387290	-0.023047	2.378030
119.157248	1802.507770	5.392294	-0.023175	2.382848
119.421904	1810.577387	5.397299	-0.023229	2.387653
119.863611	1818.679915	5.402304	-0.023317	2.392482
120.290995	1826.727987	5.407309	-0.023402	2.397267
120.770191	1834.763516	5.412314	-0.023496	2.402040
121.264386	1842.828766	5.417318	-0.023594	2.406821
121.417014	1850.914800	5.422323	-0.023627	2.411579
121.753419	1859.001587	5.427328	-0.023695	2.416342
121.991400	1867.061743	5.432333	-0.023745	2.421072
122.287225	1875.110891	5.437338	-0.023805	2.425791
122.788454	1883.194924	5.442342	-0.023904	2.430537
123.227767	1891.296813	5.447347	-0.023991	2.435279
123.556876	1899.335027	5.452352	-0.024057	2.439967
123.665391	1907.378267	5.457357	-0.024083	2.444632
124.191899	1915.406916	5.462362	-0.024186	2.449310
124.310385	1923.509125	5.467366	-0.024213	2.453992
124.435824	1931.571147	5.472371	-0.024242	2.458642
124.980760	1939.581690	5.477376	-0.024349	2.463285
125.276649	1947.650039	5.482381	-0.024409	2.467934
125.484956	1955.737575	5.487386	-0.024453	2.472578
125.943204	1963.766345	5.492390	-0.024544	2.477198
126.180919	1971.808658	5.497395	-0.024593	2.481802
126.491460	1979.878573	5.502400	-0.024656	2.486417
126.736744	1987.947944	5.507405	-0.024707	2.491019
127.245175	1995.995317	5.512410	-0.024807	2.495620
127.476818	2004.091979	5.517414	-0.024855	2.500219
127.854166	2012.094466	5.522419	-0.024931	2.504767
128.265580	2020.176904	5.527424	-0.025013	2.509355
128.676584	2028.271678	5.532429	-0.025095	2.513941
128.689661	2036.332770	5.537434	-0.025102	2.518470
128.939604	2044.376905	5.542438	-0.025154	2.523000
129.322085	2052.383522	5.547443	-0.025231	2.527509
129.874646	2060.435225	5.552448	-0.025339	2.532048
130.469166	2068.474525	5.557453	-0.025455	2.536575
130.864658	2076.521381	5.562458	-0.025534	2.541083
131.259759	2084.571307	5.567462	-0.025612	2.545585
131.566667	2092.646662	5.572467	-0.025675	2.550087
131.987863	2100.725936	5.577472	-0.025758	2.554591
132.352986	2108.755624	5.582477	-0.025832	2.559056
132.878959	2116.776112	5.587482	-0.025935	2.563519
133.699238	2124.832165	5.592486	-0.026093	2.568014
134.134486	2132.878949	5.597491	-0.026179	2.572470
134.504897	2140.965764	5.602496	-0.026253	2.576935
134.574861	2149.050152	5.607501	-0.026272	2.581370
134.767557	2157.103109	5.612506	-0.026313	2.585789
135.350340	2165.168864	5.617510	-0.026427	2.590234
135.287429	2173.424466	5.622515	-0.026420	2.594731
135.677466	2181.405557	5.627520	-0.026498	2.599101
136.081342	2189.388533	5.632525	-0.026579	2.603466
136.359099	2197.401725	5.637530	-0.026635	2.607831
136.900069	2205.430130	5.642534	-0.026741	2.612215
136.996355	2213.486801	5.647539	-0.026765	2.616577
137.453040	2221.509136	5.652544	-0.026855	2.620937
137.640540	2229.568269	5.657549	-0.026895	2.625292
138.036166	2237.580340	5.662554	-0.026974	2.629628
138.559089	2245.678912	5.667558	-0.027077	2.634011
138.823224	2253.721752	5.672563	-0.027131	2.638341
139.095396	2261.754797	5.677568	-0.027187	2.642658
139.538109	2269.786939	5.682573	-0.027275	2.646979
139.693037	2277.851932	5.687578	-0.027309	2.651292
139.766616	2285.962697	5.692582	-0.027328	2.655616
140.103301	2293.965864	5.697587	-0.027396	2.659894
140.638800	2301.996715	5.702592	-0.027501	2.664192
141.013007	2310.035741	5.707597	-0.027575	2.668477
141.476585	2318.113660	5.712602	-0.027667	2.672781
141.846006	2326.168997	5.717606	-0.027741	2.677060
141.923747	2334.205858	5.722611	-0.027761	2.681304
142.136230	2342.256410	5.727616	-0.027806	2.685558
142.604477	2350.265190	5.732621	-0.027898	2.689798
142.672364	2358.355410	5.737626	-0.027916	2.694049
142.902273	2366.419872	5.742630	-0.027964	2.698291
143.167434	2374.442773	5.747635	-0.028019	2.702506
143.655810	2382.482669	5.752640	-0.028115	2.706737
143.803673	2390.560064	5.757645	-0.028148	2.710960
143.885872	2398.637007	5.762650	-0.028168	2.715172
144.469623	2406.628196	5.767654	-0.028282	2.719364
144.695676	2414.653045	5.772659	-0.028329	2.723544
145.081259	2422.716573	5.777664	-0.028406	2.727748
145.441740	2430.769799	5.782669	-0.028479	2.731939
145.665734	2438.843941	5.787674	-0.028526	2.736126
146.028108	2446.876656	5.792678	-0.028599	2.740293
146.264162	2454.884601	5.797683	-0.028648	2.744433
146.661288	2462.955000	5.802688	-0.028727	2.748609
146.748131	2471.089684	5.807693	-0.028748	2.752793
147.418944	2479.087069	5.812698	-0.028879	2.756935
147.963777	2487.097028	5.817702	-0.028985	2.761070
148.024422	2495.134545	5.822707	-0.029002	2.765184
148.334906	2503.164613	5.827712	-0.029065	2.769302
148.800840	2511.224193	5.832717	-0.029157	2.773439
148.788252	2519.275197	5.837722	-0.029160	2.777536
149.082234	2527.312211	5.842726	-0.029220	2.781639
149.239634	2535.344524	5.847731	-0.029254	2.785725
149.542719	2543.389073	5.852736	-0.029316	2.789820
149.714297	2551.476296	5.857741	-0.029353	2.793923
149.922743	2559.490249	5.862746	-0.029397	2.797984
150.471000	2567.506438	5.867750	-0.029504	2.802061
150.591954	2575.547307	5.872755	-0.029532	2.806119
150.929126	2583.591145	5.877760	-0.029600	2.810186
151.053152	2591.678790	5.882765	-0.029629	2.814256
151.576138	2599.677016	5.887770	-0.029731	2.818298
151.749264	2607.737076	5.892774	-0.029769	2.822346
151.939049	2615.779423	5.897779	-0.029809	2.826379
152.293239	2623.818983	5.902784	-0.029881	2.830415
152.780300	2631.893918	5.907789	-0.029976	2.834470
153.035334	2639.891040	5.912794	-0.030029	2.838468
153.398011	2647.923165	5.917798	-0.030102	2.842483
153.336747	2655.977801	5.922803	-0.030096	2.846480
153.605422	2664.029701	5.927808	-0.030151	2.850488
153.787903	2672.096518	5.932813	-0.030190	2.854493
154.180766	2680.093559	5.937818	-0.030269	2.858470
154.654687	2688.120668	5.942822	-0.030362	2.862461
154.977922	2696.164146	5.947827	-0.030428	2.866445
155.226900	2704.218450	5.952832	-0.030479	2.870425
155.275240	2712.294479	5.957837	-0.030493	2.874400
155.560527	2720.315786	5.962842	-0.030552	2.878355
155.811683	2728.357830	5.967846	-0.030604	2.882312
155.981961	2736.397119	5.972851	-0.030641	2.886259
156.448544	2744.413278	5.977856	-0.030733	2.890205
156.734165	2752.485052	5.982861	-0.030791	2.894163
156.934638	2760.505093	5.987866	-0.030834	2.898085
157.162606	2768.577973	5.992870	-0.030882	2.902029
157.252026	2776.597624	5.997875	-0.030903	2.905935
157.645991	2784.638923	6.002880	-0.030982	2.909862
157.813132	2792.777451	6.007885	-0.031019	2.913819
157.900734	2800.792709	6.012890	-0.031040	2.917707
158.396295	2808.774620	6.017894	-0.031138	2.921594
158.700095	2816.772262	6.022899	-0.031199	2.925474
158.900319	2824.799778	6.027904	-0.031242	2.929358
159.219437	2832.859458	6.032909	-0.031307	2.933259
159.602664	2840.877618	6.037914	-0.031383	2.937137
159.959812	2848.913973	6.042918	-0.031455	2.941018
160.335302	2856.919444	6.047923	-0.031530	2.944879
160.596885	2864.961653	6.052928	-0.031584	2.948747
160.722782	2873.068395	6.057933	-0.031613	2.952634
160.775577	2881.133005	6.062938	-0.031628	2.956492
161.124444	2889.125254	6.067942	-0.031698	2.960326
161.174998	2897.148988	6.072947	-0.031713	2.964154
161.392818	2905.197982	6.077952	-0.031758	2.967998
161.690761	2913.252235	6.082957	-0.031819	2.971843
162.077104	2921.278033	6.087962	-0.031896	2.975674
162.372924	2929.295068	6.092966	-0.031957	2.979492
162.484511	2937.340196	6.097971	-0.031983	2.983309
162.802699	2945.373724	6.102976	-0.032047	2.987125
163.223127	2953.406849	6.107981	-0.032131	2.990942
163.123669	2961.471781	6.112986	-0.032117	2.994743
163.829759	2969.469016	6.117990	-0.032254	2.998547
164.103075	2977.493264	6.122995	-0.032310	3.002337
164.128524	2985.563888	6.128000	-0.032320	3.006132
164.372561	2993.577825	6.133005	-0.032371	3.009907
164.677496	3001.628877	6.138010	-0.032433	3.013697
164.928855	3009.687839	6.143014	-0.032485	3.017483
165.046033	3017.703635	6.148019	-0.032512	3.021238
165.465237	3025.697274	6.153024	-0.032595	3.024993
165.799733	3033.760785	6.158029	-0.032663	3.028771
166.010815	3041.803803	6.163034	-0.032707	3.032529
166.308789	3049.882801	6.168038	-0.032768	3.036303
166.370385	3057.876869	6.173043	-0.032785	3.040022
166.846033	3065.874284	6.178048	-0.032879	3.043757
167.128625	3073.927981	6.183053	-0.032936	3.047505
167.348186	3081.981373	6.188058	-0.032983	3.051245
167.837274	3090.019755	6.193062	-0.033079	3.054986
167.982698	3098.056858	6.198067	-0.033111	3.058705
168.352991	3106.065220	6.203072	-0.033185	3.062418
168.792921	3114.102815	6.208077	-0.033273	3.066142
169.113817	3122.129985	6.213082	-0.033338	3.069852
169.320520	3130.297593	6.218086	-0.033381	3.073616
169.798551	3138.265398	6.223091	-0.033476	3.077297
170.202921	3146.275672	6.228096	-0.033556	3.080989
170.337555	3154.278067	6.233101	-0.033586	3.084660
170.717585	3162.300096	6.238106	-0.033662	3.088347
170.809404	3170.390385	6.243110	-0.033685	3.092048
171.205641	3178.400222	6.248115	-0.033764	3.095722
171.315496	3186.427312	6.253120	-0.033789	3.099386
171.680177	3194.444585	6.258125	-0.033863	3.103053
171.790350	3202.489450	6.263130	-0.033888	3.106716
171.890317	3210.557273	6.268134	-0.033912	3.110385
172.210621	3218.562448	6.273139	-0.033977	3.114031
172.405162	3226.608301	6.278144	-0.034019	3.117686
172.532405	3234.648988	6.283149	-0.034047	3.121331
172.971575	3242.608111	6.288154	-0.034134	3.124949
173.274242	3250.671131	6.293158	-0.034196	3.128603
173.233585	3258.732612	6.298163	-0.034194	3.132237
173.557913	3266.782043	6.303168	-0.034259	3.135877
174.013156	3274.778834	6.308173	-0.034349	3.139496
174.178819	3282.770413	6.313178	-0.034385	3.143095
174.314666	3290.882715	6.318182	-0.034416	3.146743
174.522194	3298.889517	6.323187	-0.034460	3.150342
174.928550	3306.946172	6.328192	-0.034541	3.153968
175.161024	3314.974077	6.333197	-0.034589	3.157570
175.326915	3322.990477	6.338202	-0.034625	3.161159
175.672371	3330.991668	6.343206	-0.034695	3.164745
175.933879	3339.010238	6.348211	-0.034749	3.168332
176.444826	3347.060938	6.353216	-0.034849	3.171939
176.874261	3355.121901	6.358221	-0.034935	3.175543
176.909688	3363.114838	6.363226	-0.034946	3.179096
177.161084	3371.178361	6.368230	-0.034998	3.182685
177.475286	3379.186616	6.373235	-0.035062	3.186248
177.613399	3387.242703	6.378240	-0.035093	3.189822
177.651823	3395.315291	6.383245	-0.035105	3.193394
178.051238	3403.315203	6.388250	-0.035185	3.196945
178.572472	3411.312641	6.393254	-0.035287	3.200496
178.715080	3419.308359	6.398259	-0.035319	3.204027
179.170882	3427.347185	6.403264	-0.035409	3.207586
179.349150	3435.427770	6.408269	-0.035448	3.211147
179.444773	3443.449135	6.413274	-0.035471	3.214676
179.869699	3451.496088	6.418278	-0.035555	3.218225
180.241966	3459.512904	6.423283	-0.035630	3.221754
180.344580	3467.520440	6.428288	-0.035654	3.225265
180.651202	3475.576252	6.433293	-0.035716	3.228801
180.762836	3483.667818	6.438298	-0.035742	3.232341
181.078896	3491.729252	6.443302	-0.035807	3.235873
181.347245	3499.664372	6.448307	-0.035862	3.239343
181.484681	3507.681954	6.453312	-0.035892	3.242840
181.929791	3515.714279	6.458317	-0.035981	3.246353
182.262364	3523.709845	6.463322	-0.036048	3.249841
182.280883	3531.814331	6.468326	-0.036056	3.253359
182.612535	3539.829677	6.473331	-0.036123	3.256848
183.033724	3547.817451	6.478336	-0.036207	3.260325
183.121882	3555.864651	6.483341	-0.036229	3.263810
183.224874	3563.914090	6.488346	-0.036253	3.267293
183.545369	3571.954529	6.493350	-0.036318	3.270778
183.840533	3579.998041	6.498355	-0.036378	3.274258
183.918927	3588.027877	6.503360	-0.036398	3.277721
184.164772	3596.041656	6.508365	-0.036449	3.281180
184.415676	3604.009793	6.513370	-0.036501	3.284615
184.634831	3612.077996	6.518374	-0.036547	3.288089
184.829382	3620.113372	6.523379	-0.036589	3.291543
185.252530	3628.136775	6.528384	-0.036673	3.294998
185.668069	3636.144686	6.533389	-0.036755	3.298442
185.797130	3644.163399	6.538394	-0.036784	3.301877
186.043259	3652.223231	6.543398	-0.036836	3.305329
186.207410	3660.257921	6.548403	-0.036871	3.308764
186.399084	3668.318387	6.553408	-0.036912	3.312208
186.724057	3676.355731	6.558413	-0.036978	3.315643
186.916226	3684.345761	6.563418	-0.037019	3.319049
187.055479	3692.364200	6.568422	-0.037050	3.322462
187.125990	3700.378613	6.573427	-0.037069	3.325868
187.660522	3708.382636	6.578432	-0.037173	3.329282
188.023505	3716.439658	6.583437	-0.037246	3.332709
188.090826	3724.489668	6.588442	-0.037264	3.336119
188.537429	3732.495667	6.593446	-0.037352	3.339520
188.869146	3740.507473	6.598451	-0.037419	3.342916
188.981632	3748.557731	6.603456	-0.037446	3.346317
189.184132	3756.582504	6.608461	-0.037488	3.349707
189.508168	3764.636904	6.613466	-0.037554	3.353110
190.013026	3772.679601	6.618470	-0.037653	3.356512
190.052233	3780.659269	6.623475	-0.037666	3.359866
190.423451	3788.665313	6.628480	-0.037740	3.363240
190.773354	3796.735779	6.633485	-0.037811	3.366637
190.822634	3804.756754	6.638490	-0.037825	3.370000
191.411568	3812.809169	6.643494	-0.037940	3.373391
191.566910	3820.864272	6.648499	-0.037974	3.376764
191.560230	3828.866477	6.653504	-0.037978	3.380106
191.815916	3836.905294	6.658509	-0.038031	3.383469
191.910672	3844.938858	6.663514	-0.038054	3.386822
192.421153	3852.943144	6.668518	-0.038154	3.390173
192.407948	3861.061952	6.673523	-0.038157	3.393550
192.687634	3869.062815	6.678528	-0.038214	3.396885
192.985162	3877.040846	6.683533	-0.038275	3.400207
193.156180	3885.011034	6.688538	-0.038312	3.403519
193.566009	3893.048326	6.693542	-0.038393	3.406864
193.873150	3901.049434	6.698547	-0.038456	3.410187
193.989818	3909.136223	6.703552	-0.038483	3.413535
194.209343	3917.184705	6.708557	-0.038529	3.416868
194.148191	3925.177291	6.713562	-0.038523	3.420165
194.444959	3933.192790	6.718566	-0.038583	3.423480
194.582851	3941.211058	6.723571	-0.038614	3.426788
194.739688	3949.246976	6.728576	-0.038649	3.430100
195.103090	3957.304246	6.733581	-0.038721	3.433425
195.183375	3965.359132	6.738586	-0.038742	3.436736
195.423575	3973.338793	6.743590	-0.038792	3.440019
195.552424	3981.339803	6.748595	-0.038821	3.443303
195.827337	3989.375587	6.753600	-0.038877	3.446603
195.951518	3997.415353	6.758605	-0.038906	3.449897
196.288739	4005.448758	6.763610	-0.038974	3.453192
196.621360	4013.490370	6.768614	-0.039041	3.456487
196.695418	4021.505430	6.773619	-0.039060	3.459759
196.975954	4029.491678	6.778624	-0.039117	3.463024
197.176350	4037.594011	6.783629	-0.039160	3.466330
197.038020	4045.582195	6.788634	-0.039139	3.469575
197.512754	4053.653614	6.793638	-0.039233	3.472871
197.964924	4061.682410	6.798643	-0.039322	3.476145
198.047035	4069.645830	6.803648	-0.039343	3.479379
198.229605	4077.691246	6.808653	-0.039382	3.482645
198.383094	4085.669453	6.813658	-0.039416	3.485881
198.604172	4093.730922	6.818662	-0.039462	3.489149
198.800934	4101.748634	6.823667	-0.039504	3.492395
198.880817	4109.798498	6.828672	-0.039524	3.495648
199.271374	4117.803070	6.833677	-0.039602	3.498889
199.745828	4125.782385	6.838682	-0.039696	3.502120
199.878486	4133.825248	6.843686	-0.039726	3.505362
200.144438	4141.869209	6.848691	-0.039781	3.508607
200.406825	4149.894596	6.853696	-0.039835	3.511840
200.890200	4157.956417	6.858701	-0.039930	3.515092
201.030239	4165.926120	6.863706	-0.039961	3.518293
201.255201	4173.970696	6.868710	-0.040008	3.521524
201.349016	4181.992211	6.873715	-0.040031	3.524739
201.645817	4190.013462	6.878720	-0.040092	3.527957
201.987839	4198.048908	6.883725	-0.040160	3.531179
201.975240	4206.103057	6.888730	-0.040163	3.534394
202.190457	4214.143426	6.893734	-0.040209	3.537608
202.406905	4222.150371	6.898739	-0.040254	3.540806
202.690378	4230.150998	6.903744	-0.040312	3.544001
202.774054	4238.210063	6.908749	-0.040333	3.547209
203.026730	4246.233195	6.913754	-0.040385	3.550406
203.526510	4254.338072	6.918758	-0.040484	3.553640
203.717821	4262.356202	6.923763	-0.040525	3.556826
203.704639	4270.318773	6.928768	-0.040527	3.559983
204.082296	4278.326543	6.933773	-0.040603	3.563165
204.252232	4286.332501	6.938778	-0.040640	3.566338
204.564963	4294.364402	6.943782	-0.040703	3.569522
204.850340	4302.404841	6.948787	-0.040762	3.572707
205.047557	4310.423424	6.953792	-0.040803	3.575877
205.286682	4318.444577	6.958797	-0.040853	3.579046
205.672756	4326.435304	6.963802	-0.040930	3.582205
205.734716	4334.482185	6.968806	-0.040947	3.585374
205.796783	4342.498881	6.973811	-0.040964	3.588528
206.039909	4350.544574	6.978816	-0.041014	3.591696
206.180383	4358.584986	6.983821	-0.041046	3.594856
206.348857	4366.570803	6.988826	-0.041082	3.597993
206.617774	4374.590754	6.993830	-0.041138	3.601143
206.995769	4382.569378	6.998835	-0.041213	3.604277
207.283905	4390.599853	7.003840	-0.041272	3.607426
207.364926	4398.642602	7.008845	-0.041292	3.610571
207.586377	4406.687261	7.013850	-0.041339	3.613719
208.344086	4414.715575	7.018854	-0.041485	3.616872
208.411375	4422.710928	7.023859	-0.041503	3.619990
208.419935	4430.734180	7.028864	-0.041510	3.623115
208.786844	4438.796261	7.033869	-0.041583	3.626262
208.992002	4446.798885	7.038874	-0.041627	3.629378
209.252509	4454.882631	7.043878	-0.041681	3.632525
209.360519	4462.909256	7.048883	-0.041706	3.635643
209.810918	4470.886087	7.053888	-0.041795	3.638748
210.006782	4478.935893	7.058893	-0.041837	3.641872
210.070667	4486.919493	7.063898	-0.041854	3.644964
210.577491	4494.961858	7.068902	-0.041953	3.648088
210.809630	4502.999450	7.073907	-0.042002	3.651200
210.764738	4511.032188	7.078912	-0.041999	3.654300
211.199682	4519.072256	7.083917	-0.042085	3.657413
211.340721	4527.055865	7.088922	-0.042117	3.660494
211.507665	4535.085879	7.093926	-0.042153	3.663591
211.768418	4543.106695	7.098931	-0.042207	3.666684
211.946850	4551.136699	7.103936	-0.042245	3.669776
212.134839	4559.220894	7.108941	-0.042285	3.672886
212.339870	4567.196145	7.113946	-0.042329	3.675952
212.585046	4575.217828	7.118950	-0.042380	3.679034
212.774676	4583.237007	7.123955	-0.042420	3.682112
212.860830	4591.209477	7.128960	-0.042441	3.685166
213.207987	4599.259528	7.133965	-0.042511	3.688254
213.384738	4607.290951	7.138970	-0.042549	3.691328
213.414091	4615.331485	7.143974	-0.042560	3.694399
213.532156	4623.355724	7.148979	-0.042587	3.697463
213.764632	4631.345610	7.153984	-0.042636	3.700515
214.057190	4639.377643	7.158989	-0.042696	3.703582
214.212202	4647.388480	7.163994	-0.042730	3.706635
214.481411	4655.422416	7.168998	-0.042785	3.709696
214.636502	4663.537892	7.174003	-0.042819	3.712784
214.830482	4671.553213	7.179008	-0.042861	3.715831
215.115366	4679.524910	7.184013	-0.042919	3.718862
215.430620	4687.502122	7.189018	-0.042983	3.721893
215.533265	4695.489653	7.194022	-0.043007	3.724921
215.959653	4703.534124	7.199027	-0.043092	3.727975
216.233077	4711.553785	7.204032	-0.043148	3.731014
216.589558	4719.623640	7.209037	-0.043219	3.734071
216.827329	4727.605151	7.214042	-0.043269	3.737089
216.956118	4735.653074	7.219046	-0.043298	3.740127
217.389797	4743.687680	7.224051	-0.043384	3.743165
217.336890	4751.708796	7.229056	-0.043380	3.746184
217.461603	4759.746063	7.234061	-0.043408	3.749211
217.571342	4767.765062	7.239066	-0.043434	3.752228
218.035879	4775.801051	7.244070	-0.043525	3.755258
218.385714	4783.823352	7.249075	-0.043596	3.758277
218.536170	4791.811218	7.254080	-0.043629	3.761276
218.688670	4799.828744	7.259085	-0.043663	3.764283
218.781731	4807.889755	7.264090	-0.043685	3.767303
218.965186	4815.895844	7.269094	-0.043725	3.770303
219.182097	4823.923911	7.274099	-0.043770	3.773309
219.374030	4831.947450	7.279104	-0.043811	3.776310
219.839036	4839.946770	7.284109	-0.043903	3.779306
219.963295	4847.971453	7.289114	-0.043931	3.782301
220.176407	4855.992206	7.294118	-0.043976	3.785294
220.385789	4864.045636	7.299123	-0.044021	3.788297
220.457167	4872.051643	7.304128	-0.044039	3.791277
220.919812	4880.118916	7.309133	-0.044130	3.794286
221.020885	4888.106548	7.314138	-0.044154	3.797255
221.084826	4896.081633	7.319142	-0.044172	3.800217
221.545063	4904.096122	7.324147	-0.044263	3.803199
221.829646	4912.086092	7.329152	-0.044321	3.806166
222.032865	4920.156344	7.334157	-0.044364	3.809158
222.010831	4928.174381	7.339162	-0.044365	3.812124
222.470402	4936.191867	7.344166	-0.044456	3.815098
222.686957	4944.186732	7.349171	-0.044501	3.818055
222.961379	4952.220952	7.354176	-0.044558	3.821027
223.049757	4960.242587	7.359181	-0.044579	3.823987
223.163643	4968.289364	7.364186	-0.044606	3.826955
223.403503	4976.295402	7.369190	-0.044656	3.829908
223.647896	4984.353310	7.374195	-0.044706	3.832878
223.900281	4992.366159	7.379200	-0.044759	3.835829
224.219176	5000.358591	7.384205	-0.044823	3.838772
224.503545	5008.357539	7.389210	-0.044881	3.841714
224.784706	5016.337385	7.394214	-0.044939	3.844647
225.000529	5024.429355	7.399219	-0.044984	3.847617
225.134747	5032.423060	7.404224	-0.045015	3.850547
225.504312	5040.504609	7.409229	-0.045089	3.853512
225.459605	5048.525747	7.414234	-0.045086	3.856444
225.476248	5056.518830	7.419238	-0.045094	3.859365
226.040903	5064.558075	7.424243	-0.045204	3.862312
226.103236	5072.528429	7.429248	-0.045221	3.865221
226.272349	5080.619806	7.434253	-0.045258	3.868174
226.437789	5088.637909	7.439258	-0.045294	3.871098
226.626369	5096.878843	7.444262	-0.045334	3.874102
226.919352	5104.871617	7.449267	-0.045394	3.877014
227.047180	5112.767683	7.454272	-0.045423	3.879887
227.252572	5120.763551	7.459277	-0.045467	3.882794
227.322414	5128.691830	7.464282	-0.045485	3.885673
227.580702	5136.724542	7.469286	-0.045538	3.888591
227.978257	5144.773279	7.474291	-0.045617	3.891515
228.182280	5152.793591	7.479296	-0.045661	3.894423
228.457342	5160.809357	7.484301	-0.045717	3.897328
228.705891	5168.832617	7.489306	-0.045769	3.900233
228.927803	5176.839154	7.494310	-0.045815	3.903130
229.026610	5184.875434	7.499315	-0.045839	3.906033
229.031440	5192.874983	7.504320	-0.045845	3.908918
229.560756	5200.921013	7.509325	-0.045949	3.911828
229.666634	5208.965521	7.514330	-0.045974	3.914728
229.735528	5216.947648	7.519334	-0.045992	3.917602
230.041539	5224.960936	7.524339	-0.046054	3.920490
230.220232	5232.942408	7.529344	-0.046092	3.923361
230.574624	5240.987896	7.534349	-0.046164	3.926257
230.616888	5248.996016	7.539354	-0.046177	3.929131
230.912913	5257.033007	7.544358	-0.046237	3.932018
231.233686	5265.065215	7.549363	-0.046302	3.934902
231.321348	5273.052258	7.554368	-0.046324	3.937764
231.764889	5281.068538	7.559373	-0.046411	3.940640
231.699928	5289.105498	7.564378	-0.046404	3.943512
231.732568	5297.146118	7.569382	-0.046416	3.946385
232.009355	5305.148291	7.574387	-0.046473	3.949247
232.226442	5313.193448	7.579392	-0.046518	3.952120
232.543192	5321.259869	7.584397	-0.046582	3.955001
232.806138	5329.234091	7.589402	-0.046637	3.957846
233.079512	5337.253149	7.594406	-0.046693	3.960706
233.220492	5345.208970	7.599411	-0.046724	3.963538
233.504635	5353.190063	7.604416	-0.046782	3.966380
233.862158	5361.261442	7.609421	-0.046854	3.969252
233.903250	5369.282560	7.614426	-0.046867	3.972100
234.001546	5377.337578	7.619430	-0.046891	3.974959
234.224183	5385.398762	7.624435	-0.046937	3.977819
234.527904	5393.355349	7.629440	-0.046999	3.980642
234.908843	5401.375891	7.634445	-0.047075	3.983487
234.991692	5409.390572	7.639450	-0.047096	3.986323
235.410186	5417.429942	7.644454	-0.047179	3.989170
235.669560	5425.481687	7.649459	-0.047233	3.992018
235.638285	5433.519882	7.654464	-0.047232	3.994854
235.856853	5441.546174	7.659469	-0.047278	3.997688
236.038130	5449.508166	7.664474	-0.047317	4.000496
236.066799	5457.560796	7.669478	-0.047327	4.003333
236.388879	5465.586401	7.674483	-0.047393	4.006162
236.479953	5473.586448	7.679488	-0.047415	4.008976
236.623581	5481.653807	7.684493	-0.047447	4.011813
236.613188	5489.668870	7.689498	-0.047450	4.014627
237.159017	5497.667585	7.694502	-0.047557	4.017442
237.131429	5505.692989	7.699507	-0.047557	4.020256
237.280306	5513.675259	7.704512	-0.047590	4.023055
237.476528	5521.723525	7.709517	-0.047632	4.025876
237.799361	5529.721137	7.714522	-0.047697	4.028679
237.863648	5537.747278	7.719526	-0.047714	4.031487
238.290874	5545.896574	7.724531	-0.047799	4.034341
238.444550	5553.855162	7.729536	-0.047833	4.037122
238.611518	5561.825901	7.734541	-0.047869	4.039905
238.824596	5569.826229	7.739546	-0.047914	4.042698
238.927188	5577.806389	7.744550	-0.047938	4.045480
239.275661	5585.858863	7.749555	-0.048009	4.048289
239.172200	5593.884889	7.754560	-0.047995	4.051080
239.481464	5601.934202	7.759565	-0.048057	4.053883
239.592487	5609.930953	7.764570	-0.048083	4.056663
239.816490	5617.908779	7.769574	-0.048130	4.059436
240.006691	5625.948458	7.774579	-0.048171	4.062229
240.221587	5633.900873	7.779584	-0.048216	4.064989
240.468515	5641.990877	7.784589	-0.048267	4.067796
240.474924	5650.003446	7.789594	-0.048274	4.070570
240.756565	5658.025713	7.794598	-0.048331	4.073350
240.984187	5666.077434	7.799603	-0.048379	4.076138
240.993420	5674.046802	7.804608	-0.048386	4.078892
241.198289	5682.132253	7.809613	-0.048429	4.081686
241.489092	5690.066982	7.814618	-0.048489	4.084428
241.450621	5698.095325	7.819622	-0.048487	4.087196
241.545279	5706.096690	7.824627	-0.048510	4.089955
241.693477	5714.145850	7.829632	-0.048543	4.092729
241.864156	5722.231429	7.834637	-0.048580	4.095514
242.107860	5730.194446	7.839642	-0.048630	4.098255
242.351760	5738.213785	7.844646	-0.048681	4.101015
242.540643	5746.248015	7.849651	-0.048721	4.103776
242.707944	5754.258534	7.854656	-0.048758	4.106528
242.997833	5762.259843	7.859661	-0.048817	4.109276
243.090938	5770.330546	7.864666	-0.048839	4.112043
243.254851	5778.328396	7.869670	-0.048875	4.114785
243.436494	5786.365666	7.874675	-0.048914	4.117538
243.645717	5794.337070	7.879680	-0.048958	4.120267
243.770830	5802.342540	7.884685	-0.048987	4.123005
243.951229	5810.345875	7.889690	-0.049026	4.125741
244.202201	5818.373070	7.894694	-0.049078	4.128485
244.292563	5826.404226	7.899699	-0.049100	4.131225
244.368510	5834.452273	7.904704	-0.049119	4.133970
244.606566	5842.539302	7.909709	-0.049169	4.136728
244.951655	5850.458303	7.914714	-0.049238	4.139428
245.022505	5858.532815	7.919718	-0.049257	4.142176
245.138341	5866.516525	7.924723	-0.049283	4.144892
245.414426	5874.539416	7.929728	-0.049340	4.147621
245.561231	5882.582350	7.934733	-0.049373	4.150354
245.449209	5890.606517	7.939738	-0.049357	4.153075
245.701345	5898.645424	7.944742	-0.049409	4.155804
246.255220	5906.650786	7.949747	-0.049517	4.158524
246.292915	5914.632233	7.954752	-0.049530	4.161227
246.515303	5922.637531	7.959757	-0.049576	4.163939
246.678154	5930.699100	7.964762	-0.049612	4.166667
246.921811	5938.682923	7.969766	-0.049662	4.169368
246.989410	5946.690855	7.974771	-0.049680	4.172074
247.477450	5954.763155	7.979776	-0.049776	4.174804
247.579562	5962.790728	7.984781	-0.049801	4.177513
247.534261	5970.764473	7.989786	-0.049797	4.180200
247.790513	5978.757606	7.994790	-0.049850	4.182896
248.172089	5986.813168	7.999795	-0.049927	4.185612
248.225339	5994.796524	8.004800	-0.049942	4.188298
248.371606	6002.843360	8.009805	-0.049974	4.191005
248.440477	6010.959275	8.014810	-0.049992	4.193733
248.623712	6018.960633	8.019814	-0.050032	4.196422
248.961606	6026.876719	8.024819	-0.050100	4.199082
249.184441	6034.889104	8.029824	-0.050147	4.201771
249.726383	6042.845557	8.034829	-0.050253	4.204443
249.871374	6050.890420	8.039834	-0.050285	4.207139
249.864363	6058.934907	8.044838	-0.050289	4.209831
250.130772	6067.005162	8.049843	-0.050344	4.212534
250.408969	6074.993469	8.054848	-0.050401	4.215207
250.753840	6083.004596	8.059853	-0.050470	4.217886
250.833348	6091.015799	8.064858	-0.050490	4.220561
250.938825	6099.017313	8.069862	-0.050515	4.223232
251.094522	6107.042130	8.074867	-0.050549	4.225909
251.479634	6115.023208	8.079872	-0.050626	4.228572
251.831855	6123.090158	8.084877	-0.050697	4.231262
251.551392	6131.125314	8.089882	-0.050650	4.233933
251.649460	6139.155507	8.094886	-0.050674	4.236605
252.188169	6147.107772	8.099891	-0.050779	4.239253
252.489448	6155.125557	8.104896	-0.050840	4.241918
252.592988	6163.119267	8.109901	-0.050865	4.244573
252.854694	6171.193635	8.114906	-0.050919	4.247254
253.178778	6179.170689	8.119910	-0.050984	4.249901
253.398439	6187.296188	8.124915	-0.051031	4.252595
253.416779	6195.275863	8.129920	-0.051039	4.255237
253.841979	6203.315533	8.134925	-0.051124	4.257901
254.112689	6211.294695	8.139930	-0.051179	4.260542
254.165383	6219.324452	8.144934	-0.051194	4.263196
254.509661	6227.347711	8.149939	-0.051264	4.265849
254.469809	6235.366373	8.154944	-0.051261	4.268495
254.644141	6243.389129	8.159949	-0.051299	4.271143
254.870357	6251.430751	8.164954	-0.051346	4.273796
255.162035	6259.467249	8.169958	-0.051406	4.276446
255.354818	6267.420326	8.174963	-0.051447	4.279066
255.116804	6275.490865	8.179968	-0.051408	4.281719
255.378289	6283.455906	8.184973	-0.051462	4.284340
255.646209	6291.483748	8.189978	-0.051517	4.286981
255.652665	6299.475598	8.194982	-0.051523	4.289605
256.005378	6307.566590	8.199987	-0.051594	4.292264
256.237357	6315.556206	8.204992	-0.051643	4.294886
256.279828	6323.572546	8.209997	-0.051656	4.297514
256.307683	6331.573198	8.215002	-0.051666	4.300135
256.617933	6339.572970	8.220006	-0.051729	4.302757
256.794557	6347.621956	8.225011	-0.051768	4.305392
256.748318	6355.631516	8.230016	-0.051764	4.308011
257.097178	6363.648217	8.235021	-0.051834	4.310633
257.320933	6371.704388	8.240026	-0.051881	4.313266
257.280374	6379.685512	8.245030	-0.051879	4.315871
257.540866	6387.724938	8.250035	-0.051933	4.318495
257.672816	6395.700408	8.255040	-0.051962	4.321096
257.957465	6403.679258	8.260045	-0.052021	4.323697
257.925945	6411.735241	8.265050	-0.052020	4.326320
258.222939	6419.719814	8.270054	-0.052081	4.328921
258.418998	6427.799854	8.275059	-0.052122	4.331550
258.511098	6435.836199	8.280064	-0.052145	4.334162
258.719995	6443.863410	8.285069	-0.052189	4.336771
258.967157	6451.788911	8.290074	-0.052240	4.339345
259.077186	6459.837611	8.295078	-0.052266	4.341957
259.515893	6467.842978	8.300083	-0.052353	4.344556
259.678153	6475.871527	8.305088	-0.052388	4.347158
259.776180	6483.920732	8.310093	-0.052412	4.349765
260.040839	6491.959878	8.315098	-0.052466	4.352369
260.137751	6499.990882	8.320102	-0.052489	4.354967
260.140027	6508.009276	8.325107	-0.052495	4.357559
260.322963	6515.939015	8.330112	-0.052534	4.360122
260.536213	6523.972543	8.335117	-0.052579	4.362717
260.850547	6531.943194	8.340122	-0.052643	4.365290
260.991109	6539.951034	8.345126	-0.052674	4.367873
260.920797	6548.034499	8.350131	-0.052667	4.370478
261.171569	6556.044080	8.355136	-0.052718	4.373059
261.614682	6564.100564	8.360141	-0.052806	4.375655
261.574776	6572.074698	8.365146	-0.052804	4.378220
261.761834	6580.046502	8.370150	-0.052844	4.380785
262.326040	6588.079518	8.375155	-0.052954	4.383369
262.391908	6596.095163	8.380160	-0.052972	4.385943
262.539573	6604.139427	8.385165	-0.053005	4.388526
262.643053	6612.172705	8.390170	-0.053029	4.391103
262.699187	6620.185254	8.395174	-0.053045	4.393672
262.897390	6628.243997	8.400179	-0.053087	4.396255
263.324541	6636.182812	8.405184	-0.053172	4.398799
263.585316	6644.246249	8.410189	-0.053225	4.401380
263.404295	6652.230891	8.415194	-0.053197	4.403933
263.544123	6660.246219	8.420198	-0.053228	4.406495
263.869859	6668.252574	8.425203	-0.053294	4.409055
263.900388	6676.320187	8.430208	-0.053305	4.411630
264.215444	6684.361708	8.435213	-0.053369	4.414197
264.642629	6692.373033	8.440218	-0.053454	4.416754
264.891655	6700.335024	8.445222	-0.053505	4.419293
265.243514	6708.422738	8.450227	-0.053576	4.421870
265.483219	6716.353119	8.455232	-0.053626	4.424395
265.632720	6724.464179	8.460237	-0.053659	4.426976
265.588216	6732.479675	8.465242	-0.053656	4.429525
265.623837	6740.499631	8.470246	-0.053668	4.432073
265.932172	6748.522400	8.475251	-0.053730	4.434622
265.879412	6756.516490	8.480256	-0.053726	4.437159
266.054906	6764.476615	8.485261	-0.053764	4.439685
266.358479	6772.549974	8.490266	-0.053825	4.442246
266.581764	6780.463582	8.495270	-0.053872	4.444754
266.971102	6788.547268	8.500275	-0.053950	4.447315
266.885883	6796.555967	8.505280	-0.053939	4.449849
267.265107	6804.594978	8.510285	-0.054015	4.452393
267.392693	6812.612213	8.515290	-0.054044	4.454928
267.722648	6820.633591	8.520294	-0.054111	4.457463
267.952607	6828.631197	8.525299	-0.054159	4.459989
267.856436	6836.610550	8.530304	-0.054146	4.462507
267.933414	6844.655749	8.535309	-0.054166	4.465045
268.204260	6852.678590	8.540314	-0.054221	4.467574
268.523538	6860.688700	8.545318	-0.054286	4.470099
268.610565	6868.744705	8.550323	-0.054308	4.472635
268.649970	6876.746292	8.555328	-0.054320	4.475153
269.146279	6884.731682	8.560333	-0.054418	4.477666
269.106340	6892.775027	8.565338	-0.054416	4.480194
269.118873	6900.774652	8.570343	-0.054423	4.482707
269.311208	6908.780958	8.575347	-0.054464	4.485221
269.345480	6916.774481	8.580352	-0.054476	4.487729
269.612420	6924.813081	8.585357	-0.054531	4.490251
269.763829	6932.880318	8.590362	-0.054564	4.492780
269.822251	6940.860308	8.595367	-0.054580	4.495280
270.203180	6948.883754	8.600371	-0.054656	4.497793
270.261312	6956.871779	8.605376	-0.054672	4.500292
270.545265	6964.877304	8.610381	-0.054730	4.502796
270.750078	6972.874084	8.615386	-0.054774	4.505296
270.619396	6980.915154	8.620391	-0.054755	4.507807
271.172799	6988.943150	8.625395	-0.054863	4.510315
271.284706	6997.031357	8.630400	-0.054889	4.512839
271.290190	7005.083899	8.635405	-0.054895	4.515350
271.584279	7013.000498	8.640410	-0.054955	4.517818
271.723826	7020.968791	8.645415	-0.054987	4.520300
271.932015	7029.026307	8.650419	-0.055031	4.522809
272.049848	7036.985628	8.655424	-0.055058	4.525286
272.479823	7045.045692	8.660429	-0.055143	4.527793
272.647905	7053.027697	8.665434	-0.055180	4.530274
272.747335	7061.072895	8.670439	-0.055203	4.532773
272.765905	7069.129110	8.675443	-0.055212	4.535274
272.920956	7077.106448	8.680448	-0.055246	4.537749
273.145039	7085.098893	8.685453	-0.055293	4.540228
273.444327	7093.161888	8.690458	-0.055354	4.542728
273.531817	7101.100525	8.695463	-0.055375	4.545187
273.845507	7109.202728	8.700467	-0.055439	4.547696
273.796448	7117.149842	8.705472	-0.055435	4.550155
273.995678	7125.244471	8.710477	-0.055478	4.552658
274.060820	7133.258369	8.715482	-0.055495	4.555135
273.950770	7141.295621	8.720487	-0.055480	4.557618
274.352789	7149.228885	8.725491	-0.055560	4.560068
274.603344	7157.248144	8.730496	-0.055612	4.562543
274.809158	7165.273043	8.735501	-0.055655	4.565018
275.026436	7173.361108	8.740506	-0.055701	4.567511
275.462548	7181.306973	8.745511	-0.055787	4.569959
275.725358	7189.447496	8.750515	-0.055842	4.572466
275.727444	7197.385336	8.755520	-0.055847	4.574908
276.036069	7205.467708	8.760525	-0.055910	4.577395
276.344845	7213.424563	8.765530	-0.055972	4.579841
276.333448	7221.449590	8.770535	-0.055976	4.582306
276.520933	7229.419515	8.775539	-0.056016	4.584753
276.823703	7237.445445	8.780544	-0.056077	4.587217
277.090010	7245.440247	8.785549	-0.056132	4.589669
277.142506	7253.541651	8.790554	-0.056147	4.592153
277.492405	7261.553276	8.795559	-0.056218	4.594607
277.590949	7269.574737	8.800563	-0.056241	4.597064
277.709994	7277.487256	8.805568	-0.056268	4.599486
278.123525	7285.582407	8.810573	-0.056351	4.601962
278.135512	7293.543430	8.815578	-0.056358	4.604396
278.184221	7301.574068	8.820583	-0.056372	4.606850
278.608826	7309.603806	8.825587	-0.056457	4.609302
278.620363	7317.573564	8.830592	-0.056464	4.611735
279.012468	7325.615154	8.835597	-0.056542	4.614188
279.052130	7333.685647	8.840602	-0.056555	4.616649
279.261054	7341.630419	8.845607	-0.056599	4.619070
279.357257	7349.699323	8.850611	-0.056622	4.621527
279.371859	7357.609387	8.855616	-0.056630	4.623935
279.841242	7365.697547	8.860621	-0.056723	4.626396
280.172957	7373.709926	8.865626	-0.056790	4.628833
280.230715	7381.760158	8.870631	-0.056806	4.631279
280.683717	7389.820489	8.875635	-0.056895	4.633728
280.860054	7397.794229	8.880640	-0.056933	4.636148
280.992757	7405.756685	8.885645	-0.056963	4.638565
281.053202	7413.772610	8.890650	-0.056980	4.640996
281.328402	7421.778878	8.895655	-0.057036	4.643422
281.546860	7429.814036	8.900659	-0.057082	4.645857
281.714631	7437.839948	8.905664	-0.057119	4.648287
281.847791	7445.844232	8.910669	-0.057149	4.650709
282.011237	7453.893109	8.915674	-0.057184	4.653144
282.225740	7461.890672	8.920679	-0.057230	4.655561
282.462455	7469.926668	8.925683	-0.057279	4.657989
282.427045	7477.873885	8.930688	-0.057277	4.660390
282.496049	7485.944585	8.935693	-0.057296	4.662826
282.491997	7493.921935	8.940698	-0.057300	4.665232
282.840289	7501.936038	8.945703	-0.057370	4.667649
282.950757	7509.986494	8.950707	-0.057396	4.670075
282.976599	7518.053221	8.955712	-0.057406	4.672504
283.190033	7526.116807	8.960717	-0.057451	4.674932
283.490303	7534.101065	8.965722	-0.057512	4.677334
283.585023	7542.025103	8.970727	-0.057535	4.679717
283.864289	7550.074765	8.975731	-0.057592	4.682136
283.928339	7557.966351	8.980736	-0.057609	4.684507
283.936615	7566.089381	8.985741	-0.057616	4.686946
284.047848	7574.063298	8.990746	-0.057642	4.689339
284.247344	7582.104362	8.995751	-0.057684	4.691751
284.412595	7590.131717	9.000755	-0.057720	4.694157
284.633401	7598.139671	9.005760	-0.057767	4.696557
284.712266	7606.117460	9.010765	-0.057787	4.698946
285.031989	7614.187655	9.015770	-0.057851	4.701361
285.012637	7622.142743	9.020775	-0.057853	4.703741
285.073894	7630.203760	9.025779	-0.057870	4.706152
285.227940	7638.153690	9.030784	-0.057904	4.708528
285.612027	7646.225556	9.035789	-0.057980	4.710938
285.685783	7654.330566	9.040794	-0.057999	4.713358
285.742049	7662.268024	9.045799	-0.058015	4.715727
285.887359	7670.333797	9.050803	-0.058047	4.718132
285.863389	7678.253535	9.055808	-0.058048	4.720493
286.141817	7686.325602	9.060813	-0.058105	4.722898
286.487490	7694.339598	9.065818	-0.058175	4.725284
286.610909	7702.327394	9.070823	-0.058203	4.727661
286.804325	7710.383956	9.075827	-0.058244	4.730058
286.901431	7718.419600	9.080832	-0.058268	4.732447
287.032071	7726.410300	9.085837	-0.058297	4.734822
287.233752	7734.478318	9.090842	-0.058340	4.737218
287.427726	7742.383201	9.095847	-0.058381	4.739564
287.766258	7750.513522	9.100851	-0.058449	4.741976
288.005702	7758.443870	9.105856	-0.058499	4.744327
288.216527	7766.444301	9.110861	-0.058544	4.746699
288.219050	7774.519237	9.115866	-0.058549	4.749091
288.303096	7782.521144	9.120871	-0.058570	4.751461
288.485626	7790.596785	9.125875	-0.058610	4.753851
288.926209	7798.567691	9.130880	-0.058697	4.756208
289.000912	7806.566909	9.135885	-0.058716	4.758573
289.082386	7814.592412	9.140890	-0.058736	4.760945
289.231746	7822.526593	9.145895	-0.058769	4.763288
289.648658	7830.621420	9.150899	-0.058852	4.765677
289.637319	7838.577517	9.155904	-0.058855	4.768025
289.815561	7846.598193	9.160909	-0.058894	4.770390
289.982753	7854.647144	9.165914	-0.058930	4.772762
290.124388	7862.662745	9.170919	-0.058962	4.775124
290.310731	7870.696757	9.175923	-0.059002	4.777489
290.281946	7878.652349	9.180928	-0.059001	4.779831
290.691139	7886.721885	9.185933	-0.059083	4.782204
290.834814	7894.663399	9.190938	-0.059115	4.784539
290.895493	7902.702228	9.195943	-0.059131	4.786902
291.121420	7910.729366	9.200947	-0.059179	4.789259
291.254764	7918.793235	9.205952	-0.059209	4.791627
291.501574	7926.781965	9.210957	-0.059260	4.793970
291.696037	7934.853759	9.215962	-0.059301	4.796337
291.880185	7942.751612	9.220967	-0.059341	4.798652
292.128956	7950.846142	9.225971	-0.059392	4.801024
292.110477	7958.798838	9.230976	-0.059394	4.803353
292.337053	7966.827512	9.235981	-0.059442	4.805703
292.447960	7974.849831	9.240986	-0.059468	4.808050
292.521346	7982.828539	9.245991	-0.059486	4.810383
292.806661	7990.467468	9.250995	-0.059545	4.812615
292.914169	7995.134445	9.256000	-0.059568	4.813979
293.007424	7997.735708	9.261005	-0.059587	4.814738
292.933401	7999.064964	9.266010	-0.059574	4.815127
293.246280	7999.434565	9.271015	-0.059632	4.815233
293.328281	8000.580573	9.276019	-0.059648	4.815568
293.136320	8000.477997	9.281024	-0.059612	4.815539
293.363210	8000.602528	9.286029	-0.059655	4.815574
293.392564	8000.472621	9.291034	-0.059660	4.815536
293.195436	8000.589063	9.296039	-0.059624	4.815571
293.471384	8000.514541	9.301043	-0.059675	4.815548
293.568398	8000.500116	9.306048	-0.059693	4.815543
293.657761	8000.597789	9.311053	-0.059710	4.815571
293.744449	8000.509444	9.316058	-0.059726	4.815545
293.724288	8000.581790	9.321063	-0.059722	4.815566
293.990311	8000.476108	9.326067	-0.059771	4.815534
293.737219	8000.511463	9.331072	-0.059724	4.815546
293.846208	8000.585948	9.336077	-0.059745	4.815567
294.140068	8000.491415	9.341082	-0.059799	4.815538
293.992564	8000.591579	9.346087	-0.059772	4.815568
294.256566	8000.516859	9.351091	-0.059821	4.815545
294.212322	8000.501163	9.356096	-0.059813	4.815540
294.085690	8000.506548	9.361101	-0.059789	4.815542
294.244546	8000.457876	9.366106	-0.059819	4.815528
294.395843	8000.413354	9.371111	-0.059847	4.815514
294.409482	8000.341969	9.376115	-0.059849	4.815493
294.186962	8000.407758	9.381120	-0.059808	4.815513
294.382763	8000.372523	9.386125	-0.059845	4.815502
294.455672	8000.463512	9.391130	-0.059858	4.815528
294.430031	8000.447056	9.396135	-0.059853	4.815523
294.426718	8000.503649	9.401139	-0.059853	4.815540
294.439119	8000.479272	9.406144	-0.059855	4.815533
294.589959	8000.512767	9.411149	-0.059883	4.815542
294.851818	8000.519243	9.416154	-0.059932	4.815542
294.881823	8000.592421	9.421159	-0.059938	4.815564
294.876564	8000.508965	9.426163	-0.059937	4.815539
294.599498	8000.500100	9.431168	-0.059885	4.815538
294.702832	8000.536015	9.436173	-0.059904	4.815548
294.844035	8000.493463	9.441178	-0.059931	4.815535
294.875306	8000.504670	9.446183	-0.059936	4.815538
295.032777	8000.410015	9.451187	-0.059966	4.815510
295.081180	8000.428987	9.456192	-0.059975	4.815515
295.042913	8000.472176	9.461197	-0.059968	4.815528
295.006064	8000.417055	9.466202	-0.059961	4.815512
295.061039	8000.579362	9.471207	-0.059971	4.815559
295.086344	8000.423730	9.476211	-0.059976	4.815513
295.032269	8000.499791	9.481216	-0.059966	4.815536
295.084265	8000.502791	9.486221	-0.059975	4.815537
295.154269	8000.517846	9.491226	-0.059988	4.815541
295.058646	8000.518400	9.496231	-0.059971	4.815541
295.046616	8000.325810	9.501235	-0.059968	4.815485
295.048790	8000.491516	9.506240	-0.059969	4.815533
295.111893	8000.374990	9.511245	-0.059980	4.815499
295.340949	8000.411919	9.516250	-0.060023	4.815509
295.195552	8000.374239	9.521255	-0.059996	4.815498
295.354375	8000.410004	9.526259	-0.060026	4.815508
295.206983	8000.470625	9.531264	-0.059998	4.815527
295.221143	8000.609810	9.536269	-0.060001	4.815567
295.351538	8000.444162	9.541274	-0.060025	4.815518
295.266001	8000.399991	9.546279	-0.060009	4.815506
295.324100	8000.470429	9.551283	-0.060020	4.815526
295.604012	8000.468654	9.556288	-0.060072	4.815524
295.542490	8000.427019	9.561293	-0.060061	4.815512
295.371622	8000.376090	9.566298	-0.060029	4.815498
295.284902	8000.505053	9.571303	-0.060013	4.815536
295.680573	8000.409000	9.576307	-0.060086	4.815506
295.645001	8000.498195	9.581312	-0.060080	4.815532
295.385281	8000.488547	9.586317	-0.060031	4.815531
295.489445	8000.212374	9.591322	-0.060051	4.815450
295.407280	8000.514565	9.596327	-0.060036	4.815538
295.535669	8000.278339	9.601331	-0.060059	4.815469
295.577261	8000.416910	9.606336	-0.060067	4.815509
295.549293	8000.436755	9.611341	-0.060062	4.815515
295.655954	8000.323087	9.616346	-0.060082	4.815481
295.621096	8000.395192	9.621351	-0.060075	4.815503
295.529702	8000.228007	9.626355	-0.060058	4.815454
295.277392	8000.414081	9.631360	-0.060011	4.815510
295.615711	8000.401517	9.636365	-0.060074	4.815504
295.763195	8000.503365	9.641370	-0.060102	4.815533
295.548788	8000.519051	9.646375	-0.060062	4.815539
295.419550	8000.362996	9.651379	-0.060038	4.815494
295.717306	8000.480159	9.656384	-0.060093	4.815527
295.837192	8000.307923	9.661389	-0.060116	4.815476
295.716716	8000.403193	9.666394	-0.060093	4.815504
295.564507	8000.357917	9.671399	-0.060065	4.815492
295.795042	8000.376701	9.676403	-0.060108	4.815496
295.746049	8000.520185	9.681408	-0.060099	4.815538
295.642922	8000.523821	9.686413	-0.060080	4.815540
295.816239	8000.415532	9.691418	-0.060112	4.815508
295.825841	8000.607018	9.696423	-0.060114	4.815563
296.032896	8000.283378	9.701427	-0.060152	4.815468
295.778542	8000.491867	9.706432	-0.060105	4.815530
295.707237	8000.513131	9.711437	-0.060092	4.815537
295.703119	8000.373043	9.716442	-0.060091	4.815496
295.660200	8000.412949	9.721447	-0.060083	4.815508
295.844621	8000.418143	9.726451	-0.060117	4.815508
295.780681	8000.445943	9.731456	-0.060105	4.815517
295.755635	8000.311922	9.736461	-0.060100	4.815478
295.869430	8000.390765	9.741466	-0.060122	4.815500
295.804621	8000.412137	9.746471	-0.060110	4.815507
295.679055	8000.531907	9.751475	-0.060086	4.815542
295.852121	8000.382997	9.756480	-0.060118	4.815498
295.830497	8000.536555	9.761485	-0.060115	4.815543
295.820103	8000.348264	9.766490	-0.060113	4.815488
295.626433	8000.517141	9.771495	-0.060077	4.815538
295.996368	8000.289192	9.776499	-0.060145	4.815470
296.089208	8000.433958	9.781504	-0.060163	4.815512
295.849615	8000.377614	9.786509	-0.060118	4.815496
295.989063	8000.207839	9.791514	-0.060144	4.815446
295.953108	8000.413533	9.796519	-0.060137	4.815506
296.167932	8000.399992	9.801523	-0.060177	4.815501
296.258752	8000.485938	9.806528	-0.060194	4.815526
296.276707	8000.401795	9.811533	-0.060198	4.815501
296.207935	8000.313009	9.816538	-0.060185	4.815476
296.058343	8000.530717	9.821543	-0.060157	4.815540
296.151831	8000.400796	9.826547	-0.060174	4.815502
296.073273	8000.450800	9.831552	-0.060160	4.815517
296.040152	8000.580653	9.836557	-0.060154	4.815555
296.133414	8000.342773	9.841562	-0.060171	4.815485
296.096315	8000.464009	9.846567	-0.060164	4.815520
296.147147	8000.522571	9.851571	-0.060174	4.815537
296.137097	8000.348180	9.856576	-0.060172	4.815486
296.120562	8000.529613	9.861581	-0.060169	4.815539
296.166544	8000.514343	9.866586	-0.060177	4.815535
296.057568	8000.512537	9.871591	-0.060157	4.815535
296.156673	8000.297200	9.876595	-0.060175	4.815471
296.388664	8000.521232	9.881600	-0.060219	4.815536
296.179264	8000.520968	9.886605	-0.060180	4.815537
296.273605	8000.543910	9.891610	-0.060197	4.815543
296.338677	8000.516129	9.896615	-0.060209	4.815534
296.198567	8000.539460	9.901619	-0.060183	4.815542
296.053724	8000.381005	9.906624	-0.060156	4.815496
296.090668	8000.522708	9.911629	-0.060163	4.815537
296.332239	8000.524575	9.916634	-0.060208	4.815537
296.167722	8000.395722	9.921639	-0.060177	4.815500
296.252231	8000.196177	9.926643	-0.060193	4.815441
296.365932	8000.361597	9.931648	-0.060214	4.815489
296.532920	8000.362228	9.936653	-0.060245	4.815488
296.388249	8000.513748	9.941658	-0.060219	4.815533
296.277084	8000.403950	9.946663	-0.060198	4.815502
296.227829	8000.405272	9.951667	-0.060189	4.815503
296.311751	8000.523170	9.956672	-0.060204	4.815537
296.438356	8000.527407	9.961677	-0.060228	4.815537
296.487548	8000.328343	9.966682	-0.060237	4.815479
296.268164	8000.373876	9.971687	-0.060196	4.815493
296.328587	8000.379153	9.976691	-0.060207	4.815494
296.374824	8000.380988	9.981696	-0.060216	4.815495
296.305925	8000.515594	9.986701	-0.060203	4.815534
296.323494	8000.376932	9.991706	-0.060206	4.815494
296.320406	8000.519041	9.996711	-0.060206	4.815535
296.435727	8000.416203	10.001715	-0.060227	4.815505
296.280098	8000.487376	10.006720	-0.060198	4.815526
296.481966	8000.507825	10.011725	-0.060236	4.815531
296.495059	8000.218378	10.016730	-0.060238	4.815447
296.411733	8000.537659	10.021735	-0.060223	4.815540
296.638372	8000.404600	10.026739	-0.060265	4.815500
296.617095	8000.496171	10.031744	-0.060261	4.815527
296.452803	8000.512688	10.036749	-0.060231	4.815533
296.476270	8000.410465	10.041754	-0.060235	4.815503
296.546458	8000.485382	10.046759	-0.060248	4.815524
296.569322	8000.270917	10.051763	-0.060252	4.815462
296.509522	8000.388571	10.056768	-0.060241	4.815496
296.342325	8000.478792	10.061773	-0.060210	4.815523
296.484954	8000.305862	10.066778	-0.060237	4.815472
296.298297	8000.514405	10.071783	-0.060202	4.815534
296.411519	8000.397637	10.076787	-0.060223	4.815499
296.572834	8000.394967	10.081792	-0.060253	4.815498
296.611323	8000.424465	10.086797	-0.060260	4.815506
296.526845	8000.399550	10.091802	-0.060244	4.815499
296.431023	8000.509125	10.096807	-0.060227	4.815532
296.612734	8000.502518	10.101811	-0.060260	4.815529
296.442514	8000.401360	10.106816	-0.060229	4.815500
296.283397	8000.331384	10.111821	-0.060199	4.815481
296.521191	8000.251954	10.116826	-0.060243	4.815456
296.441788	8000.453724	10.121831	-0.060229	4.815516
296.329844	8000.371703	10.126835	-0.060208	4.815492
296.594625	8000.381437	10.131840	-0.060257	4.815494
296.635472	8000.313706	10.136845	-0.060265	4.815474
296.598833	8000.191249	10.141850	-0.060258	4.815438
296.570109	8000.501815	10.146855	-0.060253	4.815529
296.456919	8000.416566	10.151859	-0.060231	4.815505
296.409184	8000.432877	10.156864	-0.060223	4.815510
296.548205	8000.512141	10.161869	-0.060249	4.815532
296.741492	8000.387080	10.166874	-0.060284	4.815495
296.373702	8000.392742	10.171879	-0.060216	4.815498
296.469799	8000.527945	10.176883	-0.060234	4.815537
296.610295	8000.418042	10.181888	-0.060260	4.815504
296.599048	8000.518331	10.186893	-0.060258	4.815534
296.478212	8000.229870	10.191898	-0.060235	4.815450
296.377896	8000.508252	10.196903	-0.060217	4.815532
296.643336	8000.419660	10.201907	-0.060266	4.815505
296.691132	8000.462139	10.206912	-0.060275	4.815517
296.549829	8000.452315	10.211917	-0.060249	4.815515
296.492962	8000.405411	10.216922	-0.060238	4.815501
296.361408	8000.394680	10.221927	-0.060214	4.815499
296.668022	8000.368765	10.226931	-0.060271	4.815490
296.720531	8000.352534	10.231936	-0.060281	4.815485
296.678016	8000.538884	10.236941	-0.060273	4.815539
296.490075	8000.208694	10.241946	-0.060238	4.815444
296.488045	8000.385023	10.246951	-0.060237	4.815495
296.537002	8000.253296	10.251955	-0.060246	4.815457
296.641523	8000.414290	10.256960	-0.060266	4.815503
296.500070	8000.275130	10.261965	-0.060239	4.815463
296.633792	8000.348961	10.266970	-0.060264	4.815484
296.556301	8000.520835	10.271975	-0.060250	4.815535
296.598772	8000.266079	10.276979	-0.060258	4.815460
296.602188	8000.510908	10.281984	-0.060259	4.815532
296.602505	8000.406163	10.286989	-0.060259	4.815501
296.697269	8000.383151	10.291994	-0.060276	4.815494
296.464068	8000.528928	10.296999	-0.060233	4.815537
296.834089	8000.500859	10.302003	-0.060302	4.815528
296.714174	8000.503147	10.307008	-0.060280	4.815529
296.772902	8000.528705	10.312013	-0.060291	4.815536
296.941455	8000.247177	10.317018	-0.060322	4.815453
296.717546	8000.522444	10.322023	-0.060280	4.815534
296.664706	8000.537601	10.327027	-0.060270	4.815539
296.718064	8000.390980	10.332032	-0.060280	4.815496
296.655430	8000.509657	10.337037	-0.060269	4.815531
296.605404	8000.334601	10.342042	-0.060259	4.815480
296.581179	8000.550114	10.347047	-0.060255	4.815543
296.600612	8000.447823	10.352051	-0.060258	4.815513
296.683179	8000.361545	10.357056	-0.060274	4.815488
296.613416	8000.361457	10.362061	-0.060261	4.815488
296.877314	8000.174504	10.367066	-0.060310	4.815432
297.003174	8000.503668	10.372071	-0.060333	4.815528
296.905301	8000.211310	10.377075	-0.060315	4.815443
296.813929	8000.344474	10.382080	-0.060298	4.815482
296.815010	8000.530478	10.387085	-0.060298	4.815536
296.966527	8000.520164	10.392090	-0.060327	4.815532
296.699423	8000.524287	10.397095	-0.060277	4.815535
296.550879	8000.525031	10.402099	-0.060249	4.815536
296.796952	8000.528042	10.407104	-0.060295	4.815536
296.666764	8000.404032	10.412109	-0.060271	4.815500
296.635405	8000.284867	10.417114	-0.060265	4.815465
296.870269	8000.398855	10.422119	-0.060309	4.815498
296.656091	8000.439129	10.427123	-0.060269	4.815510
296.764050	8000.478330	10.432128	-0.060289	4.815521
296.855117	8000.411432	10.437133	-0.060306	4.815501
296.880451	8000.344512	10.442138	-0.060311	4.815482
296.865125	8000.412667	10.447143	-0.060308	4.815502
296.836974	8000.387617	10.452147	-0.060302	4.815494
296.940282	8000.393605	10.457152	-0.060322	4.815496
296.856050	8000.492684	10.462157	-0.060306	4.815525
296.766063	8000.320172	10.467162	-0.060289	4.815475
296.874850	8000.392522	10.472167	-0.060310	4.815496
296.752925	8000.340264	10.477171	-0.060287	4.815481
296.835960	8000.382258	10.482176	-0.060302	4.815493
296.929538	8000.525971	10.487181	-0.060320	4.815534
296.931486	8000.396669	10.492186	-0.060320	4.815497
296.847543	8000.510717	10.497191	-0.060305	4.815530
296.930975	8000.521721	10.502195	-0.060320	4.815533
296.915155	8000.416708	10.507200	-0.060317	4.815503
296.782823	8000.478648	10.512205	-0.060293	4.815521
296.969204	8000.245515	10.517210	-0.060327	4.815452
297.016803	8000.509250	10.522215	-0.060336	4.815529
296.938436	8000.407475	10.527219	-0.060321	4.815500
296.839699	8000.362015	10.532224	-0.060303	4.815487
296.747601	8000.395762	10.537229	-0.060286	4.815497
296.919728	8000.507642	10.542234	-0.060318	4.815529
297.006797	8000.512293	10.547239	-0.060334	4.815530
296.863556	8000.382721	10.552243	-0.060308	4.815493
296.901098	8000.383343	10.557248	-0.060315	4.815493
296.829715	8000.471947	10.562253	-0.060301	4.815519
297.057281	8000.403036	10.567258	-0.060344	4.815498
297.097500	8000.612137	10.572263	-0.060351	4.815559
297.040843	8000.527824	10.577267	-0.060341	4.815534
297.044423	8000.351517	10.582272	-0.060341	4.815483
296.891717	8000.485803	10.587277	-0.060313	4.815523
296.970744	8000.213480	10.592282	-0.060327	4.815443
296.849182	8000.506477	10.597287	-0.060305	4.815529
296.735191	8000.388079	10.602291	-0.060284	4.815495
296.899137	8000.389728	10.607296	-0.060314	4.815495
296.871641	8000.476921	10.612301	-0.060309	4.815520
296.866104	8000.442625	10.617306	-0.060308	4.815510
297.024938	8000.377919	10.622311	-0.060338	4.815491
296.950220	8000.401265	10.627315	-0.060324	4.815498
296.911429	8000.511787	10.632320	-0.060317	4.815530
296.906768	8000.391995	10.637325	-0.060316	4.815495
297.176901	8000.414645	10.642330	-0.060366	4.815501
297.204762	8000.367007	10.647335	-0.060371	4.815487
297.035219	8000.102322	10.652339	-0.060339	4.815410
297.152307	8000.325520	10.657344	-0.060361	4.815475
296.872654	8000.292025	10.662349	-0.060309	4.815466
296.851135	8000.408177	10.667354	-0.060305	4.815500
296.846033	8000.429470	10.672359	-0.060304	4.815507
296.963801	8000.443181	10.677363	-0.060326	4.815510
296.887638	8000.385268	10.682368	-0.060312	4.815493
297.037472	8000.519226	10.687373	-0.060340	4.815532
297.391045	8000.385064	10.692378	-0.060406	4.815491
296.967071	8000.395137	10.697383	-0.060327	4.815496
296.913812	8000.372877	10.702387	-0.060317	4.815490
297.186381	8000.418014	10.707392	-0.060368	4.815502
297.108691	8000.519340	10.712397	-0.060353	4.815532
297.122095	8000.418017	10.717402	-0.060356	4.815502
297.040005	8000.526753	10.722407	-0.060341	4.815534
297.057335	8000.508869	10.727411	-0.060344	4.815529
297.087883	8000.516858	10.732416	-0.060350	4.815531
296.947680	8000.507052	10.737421	-0.060323	4.815529
297.106693	8000.308738	10.742426	-0.060353	4.815470
297.191260	8000.482231	10.747431	-0.060369	4.815520
297.013034	8000.527377	10.752435	-0.060336	4.815534
297.035214	8000.620739	10.757440	-0.060340	4.815562
296.932170	8000.533519	10.762445	-0.060321	4.815537
297.125913	8000.539939	10.767450	-0.060357	4.815537
296.949367	8000.389505	10.772455	-0.060324	4.815494
297.167073	8000.525657	10.777459	-0.060364	4.815533
297.022537	8000.504021	10.782464	-0.060337	4.815528
296.947702	8000.530572	10.787469	-0.060323	4.815536
297.109537	8000.386817	10.792474	-0.060354	4.815493
296.959732	8000.605595	10.797479	-0.060326	4.815557
297.192243	8000.546386	10.802483	-0.060369	4.815539
297.118490	8000.510958	10.807488	-0.060355	4.815529
297.176769	8000.627367	10.812493	-0.060366	4.815563
297.174444	8000.409273	10.817498	-0.060366	4.815499
297.002434	8000.429937	10.822503	-0.060334	4.815506
297.076634	8000.406583	10.827507	-0.060347	4.815499
297.045866	8000.313081	10.832512	-0.060342	4.815472
296.939495	8000.502648	10.837517	-0.060322	4.815528
297.144671	8000.468639	10.842522	-0.060360	4.815517
297.201641	8000.547614	10.847527	-0.060371	4.815539
297.167939	8000.409168	10.852531	-0.060364	4.815499
297.415528	8000.405791	10.857536	-0.060411	4.815497
297.211031	8000.539220	10.862541	-0.060373	4.815537
297.135496	8000.399011	10.867546	-0.060358	4.815496
297.199936	8000.536899	10.872551	-0.060371	4.815536
297.136299	8000.627769	10.877555	-0.060359	4.815563
297.078717	8000.448309	10.882560	-0.060348	4.815511
297.081137	8000.528517	10.887565	-0.060348	4.815534
297.360237	8000.436944	10.892570	-0.060400	4.815506
297.379236	8000.608284	10.897575	-0.060404	4.815556
297.061771	8000.562401	10.902579	-0.060345	4.815544
297.271183	8000.538083	10.907584	-0.060384	4.815536
297.329305	8000.534772	10.912589	-0.060395	4.815535
297.334308	8000.408725	10.917594	-0.060395	4.815498
297.192372	8000.399959	10.922599	-0.060369	4.815496
297.255782	8000.405286	10.927603	-0.060381	4.815498
297.461464	8000.526276	10.932608	-0.060419	4.815532
297.035304	8000.389874	10.937613	-0.060340	4.815494
297.162616	8000.498874	10.942618	-0.060364	4.815525
297.151290	8000.427071	10.947623	-0.060361	4.815504
297.251929	8000.536698	10.952627	-0.060380	4.815536
297.373710	8000.369832	10.957632	-0.060403	4.815487
297.479091	8000.449610	10.962637	-0.060423	4.815509
297.344543	8000.381107	10.967642	-0.060397	4.815490
297.399499	8000.601144	10.972647	-0.060408	4.815554
297.408491	8000.540366	10.977651	-0.060409	4.815536
297.313530	8000.441521	10.982656	-0.060392	4.815508
297.089123	8000.514761	10.987661	-0.060350	4.815530
297.367627	8000.248950	10.992666	-0.060402	4.815451
297.248536	8000.517405	10.997671	-0.060380	4.815530
297.232648	8000.424148	11.002675	-0.060377	4.815503
297.243126	8000.365533	11.007680	-0.060379	4.815486
297.244753	8000.530171	11.012685	-0.060379	4.815534
297.279649	8000.411033	11.017690	-0.060385	4.815499
297.208483	8000.519950	11.022695	-0.060372	4.815531
297.067820	8000.551822	11.027699	-0.060346	4.815541
297.274904	8000.369269	11.032704	-0.060385	4.815487
297.106840	8000.527886	11.037709	-0.060353	4.815534
297.304759	8000.486274	11.042714	-0.060390	4.815521
297.265811	8000.507007	11.047719	-0.060383	4.815527
297.315426	8000.531346	11.052723	-0.060392	4.815534
297.235042	8000.519324	11.057728	-0.060377	4.815531
297.360864	8000.410246	11.062733	-0.060401	4.815498
297.347626	8000.428198	11.067738	-0.060398	4.815504
297.349900	8000.505196	11.072743	-0.060399	4.815526
297.377567	8000.408386	11.077747	-0.060404	4.815498
297.513759	8000.375371	11.082752	-0.060429	4.815488
297.172268	8000.532181	11.087757	-0.060366	4.815535
297.180825	8000.385885	11.092762	-0.060367	4.815492
297.283763	8000.400419	11.097767	-0.060386	4.815496
297.242924	8000.422189	11.102771	-0.060379	4.815503
297.236105	8000.402836	11.107776	-0.060377	4.815497
297.281132	8000.637672	11.112781	-0.060386	4.815565
297.624575	8000.418898	11.117786	-0.060450	4.815500
297.204231	8000.402309	11.122791	-0.060371	4.815497
297.207785	8000.413057	11.127795	-0.060372	4.815500
297.395095	8000.416163	11.132800	-0.060407	4.815500
297.297219	8000.476537	11.137805	-0.060389	4.815518
297.445843	8000.222467	11.142810	-0.060416	4.815443
297.311445	8000.462878	11.147815	-0.060391	4.815514
297.203857	8000.289003	11.152819	-0.060371	4.815464
297.278581	8000.407820	11.157824	-0.060385	4.815498
297.191423	8000.414926	11.162829	-0.060369	4.815501
297.290296	8000.205995	11.167834	-0.060387	4.815439
297.242456	8000.461736	11.172839	-0.060379	4.815514
297.346564	8000.411086	11.177843	-0.060398	4.815499
297.321620	8000.337988	11.182848	-0.060393	4.815478
297.190665	8000.388193	11.187853	-0.060369	4.815493
297.259191	8000.383985	11.192858	-0.060382	4.815491
297.529432	8000.375640	11.197863	-0.060432	4.815488
297.425419	8000.535319	11.202867	-0.060413	4.815535
297.458493	8000.427909	11.207872	-0.060419	4.815503
297.354655	8000.410154	11.212877	-0.060400	4.815498
297.630783	8000.419009	11.217882	-0.060451	4.815500
297.431948	8000.409299	11.222887	-0.060414	4.815498
297.352560	8000.524493	11.227891	-0.060399	4.815532
297.383508	8000.395670	11.232896	-0.060405	4.815494
297.217853	8000.539362	11.237901	-0.060374	4.815537
297.400597	8000.372438	11.242906	-0.060408	4.815487
297.537321	8000.344776	11.247911	-0.060434	4.815478
297.518754	8000.433188	11.252915	-0.060430	4.815504
297.266878	8000.360602	11.257920	-0.060383	4.815484
297.241994	8000.517318	11.262925	-0.060379	4.815530
297.355065	8000.413372	11.267930	-0.060400	4.815499
297.393259	8000.459968	11.272935	-0.060407	4.815513
297.287423	8000.534106	11.277939	-0.060387	4.815535
297.394117	8000.365921	11.282944	-0.060407	4.815485
297.477662	8000.419682	11.287949	-0.060423	4.815501
297.387948	8000.363681	11.292954	-0.060406	4.815485
297.574584	8000.394568	11.297959	-0.060441	4.815493
297.428248	8000.542856	11.302963	-0.060413	4.815537
297.472014	8000.382179	11.307968	-0.060421	4.815490
297.286984	8000.387662	11.312973	-0.060387	4.815492
297.500487	8000.444648	11.317978	-0.060427	4.815508
297.404681	8000.445197	11.322983	-0.060409	4.815508
297.321067	8000.510083	11.327987	-0.060393	4.815528
297.442274	8000.401996	11.332992	-0.060416	4.815496
297.407656	8000.390734	11.337997	-0.060410	4.815493
297.380740	8000.521763	11.343002	-0.060405	4.815531
297.334628	8000.418384	11.348007	-0.060396	4.815501
297.441686	8000.535601	11.353011	-0.060416	4.815535
297.289609	8000.408018	11.358016	-0.060388	4.815498
297.258254	8000.512251	11.363021	-0.060382	4.815529
297.327483	8000.404371	11.368026	-0.060395	4.815497
297.349244	8000.497727	11.373031	-0.060399	4.815524
297.310610	8000.488535	11.378035	-0.060392	4.815522
297.397077	8000.246262	11.383040	-0.060407	4.815450
297.330794	8000.411910	11.388045	-0.060395	4.815499
297.381626	8000.395651	11.393050	-0.060405	4.815494
297.263279	8000.518750	11.398055	-0.060383	4.815531
297.391021	8000.557212	11.403059	-0.060407	4.815541
297.437504	8000.368787	11.408064	-0.060415	4.815486
297.367644	8000.403972	11.413069	-0.060402	4.815497
297.441563	8000.415887	11.418074	-0.060416	4.815500
297.500070	8000.407237	11.423079	-0.060427	4.815497
297.272378	8000.528523	11.428083	-0.060384	4.815533
297.491734	8000.462683	11.433088	-0.060425	4.815513
297.512963	8000.595580	11.438093	-0.060429	4.815552
297.269492	8000.269805	11.443098	-0.060384	4.815458
297.305916	8000.515185	11.448103	-0.060391	4.815529
297.483679	8000.528823	11.453107	-0.060424	4.815532
297.493217	8000.394300	11.458112	-0.060426	4.815493
297.457630	8000.435397	11.463117	-0.060419	4.815505
297.514446	8000.251421	11.468122	-0.060429	4.815451
297.612806	8000.398422	11.473127	-0.060448	4.815494
297.519488	8000.413977	11.478131	-0.060430	4.815499
297.663435	8000.328715	11.483136	-0.060457	4.815473
297.493600	8000.334450	11.488141	-0.060426	4.815476
297.549506	8000.297966	11.493146	-0.060436	4.815465
297.317802	8000.382843	11.498151	-0.060393	4.815491
297.640576	8000.545325	11.503155	-0.060453	4.815537
297.582560	8000.512296	11.508160	-0.060442	4.815527
297.256217	8000.397857	11.513165	-0.060381	4.815495
297.556806	8000.386808	11.518170	-0.060437	4.815491
297.545608	8000.525580	11.523175	-0.060435	4.815531
297.481596	8000.528794	11.528179	-0.060424	4.815532
297.433984	8000.375152	11.533184	-0.060415	4.815488
297.554002	8000.509687	11.538189	-0.060437	4.815527
297.401086	8000.374608	11.543194	-0.060408	4.815488
297.303203	8000.534388	11.548199	-0.060390	4.815535
297.315009	8000.515344	11.553203	-0.060393	4.815529
297.597817	8000.524311	11.558208	-0.060445	4.815531
297.418166	8000.437957	11.563213	-0.060412	4.815506
297.276601	8000.502951	11.568218	-0.060385	4.815526
297.484494	8000.501054	11.573223	-0.060424	4.815524
297.369066	8000.404008	11.578227	-0.060403	4.815497
297.493757	8000.183747	11.583232	-0.060426	4.815432
297.469034	8000.623723	11.588237	-0.060421	4.815560
297.351686	8000.416548	11.593242	-0.060399	4.815500
297.522507	8000.362729	11.598247	-0.060431	4.815484
297.601291	8000.496580	11.603251	-0.060446	4.815523
297.627550	8000.322785	11.608256	-0.060451	4.815472
297.481322	8000.507418	11.613261	-0.060424	4.815526
297.482436	8000.377031	11.618266	-0.060424	4.815488
297.887842	8000.516299	11.623271	-0.060499	4.815527
297.724272	8000.513587	11.628275	-0.060469	4.815527
297.534632	8000.339418	11.633280	-0.060433	4.815477
297.504261	8000.476802	11.638285	-0.060428	4.815517
297.912204	8000.542359	11.643290	-0.060504	4.815534
297.710772	8000.413956	11.648295	-0.060466	4.815498
297.498076	8000.637037	11.653299	-0.060427	4.815564
297.518526	8000.416113	11.658304	-0.060430	4.815499
297.490630	8000.632639	11.663309	-0.060425	4.815563
297.613469	8000.447618	11.668314	-0.060448	4.815508
297.666628	8000.335196	11.673319	-0.060458	4.815475
297.501292	8000.492790	11.678323	-0.060427	4.815522
297.594548	8000.406687	11.683328	-0.060445	4.815496
297.839853	8000.411824	11.688333	-0.060490	4.815497
297.885667	8000.392275	11.693338	-0.060499	4.815491
297.663075	8000.306279	11.698343	-0.060457	4.815467
297.704921	8000.417070	11.703347	-0.060465	4.815499
297.924756	8000.244347	11.708352	-0.060506	4.815447
297.598815	8000.539304	11.713357	-0.060446	4.815535
297.696629	8000.400900	11.718362	-0.060464	4.815494
297.895076	8000.335781	11.723367	-0.060501	4.815474
297.814452	8000.414613	11.728371	-0.060486	4.815498
298.029893	8000.389325	11.733376	-0.060526	4.815489
297.884590	8000.302473	11.738381	-0.060499	4.815464
297.873227	8000.443380	11.743386	-0.060497	4.815506
297.793112	8000.421743	11.748391	-0.060482	4.815500
297.545944	8000.478572	11.753395	-0.060436	4.815518
297.828659	8000.274824	11.758400	-0.060488	4.815457
297.650662	8000.516652	11.763405	-0.060455	4.815528
297.636155	8000.433037	11.768410	-0.060452	4.815504
297.869639	8000.514940	11.773415	-0.060496	4.815527
297.819096	8000.517309	11.778419	-0.060487	4.815528
297.924867	8000.411104	11.783424	-0.060506	4.815496
297.734052	8000.415422	11.788429	-0.060471	4.815498
297.790194	8000.536071	11.793434	-0.060481	4.815533
297.774063	8000.429982	11.798439	-0.060478	4.815502
297.811916	8000.521467	11.803443	-0.060485	4.815529
297.849919	8000.435516	11.808448	-0.060492	4.815503
297.900167	8000.466280	11.813453	-0.060502	4.815512
297.900335	8000.396804	11.818458	-0.060502	4.815492
297.970522	8000.419346	11.823463	-0.060515	4.815498
297.962759	8000.399978	11.828467	-0.060513	4.815493
297.981983	8000.357540	11.833472	-0.060517	4.815480
297.806867	8000.419840	11.838477	-0.060484	4.815499
297.823572	8000.393395	11.843482	-0.060487	4.815491
297.894269	8000.360363	11.848487	-0.060501	4.815481
297.831852	8000.409566	11.853491	-0.060489	4.815496
298.101812	8000.256915	11.858496	-0.060539	4.815450
297.783932	8000.337156	11.863501	-0.060480	4.815475
297.733999	8000.225163	11.868506	-0.060471	4.815443
297.765240	8000.387085	11.873511	-0.060477	4.815490
297.719005	8000.401283	11.878515	-0.060468	4.815494
297.883078	8000.254358	11.883520	-0.060498	4.815450
298.010364	8000.400772	11.888525	-0.060522	4.815493
298.055635	8000.423970	11.893530	-0.060531	4.815499
297.858094	8000.388627	11.898535	-0.060494	4.815490
297.805950	8000.414485	11.903539	-0.060484	4.815498
297.867747	8000.237004	11.908544	-0.060496	4.815445
297.813605	8000.384684	11.913549	-0.060486	4.815489
297.829311	8000.396702	11.918554	-0.060489	4.815492
297.838265	8000.526190	11.923559	-0.060490	4.815530
297.928265	8000.434687	11.928563	-0.060507	4.815503
297.905974	8000.344530	11.933568	-0.060503	4.815477
297.895962	8000.383914	11.938573	-0.060501	4.815488
297.837718	8000.416084	11.943578	-0.060490	4.815498
297.948496	8000.391199	11.948583	-0.060511	4.815490
297.963850	8000.339078	11.953587	-0.060514	4.815475
298.049954	8000.387538	11.958592	-0.060530	4.815488
297.942980	8000.427452	11.963597	-0.060510	4.815501
297.922118	8000.235772	11.968602	-0.060506	4.815445
297.934433	8000.258424	11.973607	-0.060508	4.815451
297.689526	8000.552587	11.978611	-0.060463	4.815538
297.898534	8000.434198	11.983616	-0.060502	4.815503
297.825305	8000.376332	11.988621	-0.060488	4.815486
297.871747	8000.341829	11.993626	-0.060496	4.815476
297.866017	8000.318219	11.998631	-0.060495	4.815469
297.892063	8000.474711	12.003635	-0.060500	4.815515
297.803748	8000.393079	12.008640	-0.060484	4.815491
297.802318	8000.398400	12.013645	-0.060484	4.815493
297.766914	8000.499360	12.018650	-0.060477	4.815523
297.761433	8000.269455	12.023655	-0.060476	4.815455
297.826565	8000.456524	12.028659	-0.060488	4.815510
297.932141	8000.346040	12.033664	-0.060508	4.815477
297.665875	8000.410035	12.038669	-0.060458	4.815497
297.864539	8000.350265	12.043674	-0.060495	4.815478
297.894021	8000.438404	12.048679	-0.060501	4.815504
297.826851	8000.400948	12.053683	-0.060488	4.815493
297.997515	8000.264821	12.058688	-0.060520	4.815453
297.915087	8000.469753	12.063693	-0.060505	4.815513
297.892789	8000.404180	12.068698	-0.060500	4.815494
297.999487	8000.377090	12.073703	-0.060520	4.815486
297.853012	8000.265633	12.078707	-0.060493	4.815454
297.840919	8000.203437	12.083712	-0.060491	4.815436
297.756164	8000.384814	12.088717	-0.060475	4.815489
297.701696	8000.401013	12.093722	-0.060465	4.815494
297.971155	8000.226975	12.098727	-0.060515	4.815442
297.882137	8000.376215	12.103731	-0.060499	4.815486
297.920073	8000.279574	12.108736	-0.060506	4.815458
297.821145	8000.355964	12.113741	-0.060487	4.815480
297.819995	8000.400839	12.118746	-0.060487	4.815493
298.008214	8000.286381	12.123751	-0.060522	4.815459
297.907722	8000.398019	12.128755	-0.060503	4.815492
298.033395	8000.369106	12.133760	-0.060527	4.815483
297.672697	8000.496737	12.138765	-0.060460	4.815522
297.741033	8000.644313	12.143770	-0.060472	4.815565
297.973827	8000.286882	12.148775	-0.060516	4.815459
297.893144	8000.554910	12.153779	-0.060501	4.815538
297.889580	8000.398790	12.158784	-0.060500	4.815493
297.909934	8000.407679	12.163789	-0.060504	4.815495
297.945549	8000.382616	12.168794	-0.060510	4.815488
297.826154	8000.243817	12.173799	-0.060488	4.815448
297.810697	8000.543924	12.178803	-0.060485	4.815535
297.933087	8000.412340	12.183808	-0.060508	4.815496
297.704036	8000.495123	12.188813	-0.060466	4.815522
297.829424	8000.285560	12.193818	-0.060489	4.815460
297.962435	8000.360451	12.198823	-0.060514	4.815481
297.950717	8000.423323	12.203827	-0.060511	4.815499
298.000579	8000.429495	12.208832	-0.060521	4.815501
298.100320	8000.376635	12.213837	-0.060539	4.815485
298.135973	8000.423190	12.218842	-0.060546	4.815498
297.926353	8000.396198	12.223847	-0.060507	4.815492
297.709221	8000.374426	12.228851	-0.060466	4.815486
297.869106	8000.226363	12.233856	-0.060496	4.815442
297.603137	8000.520176	12.238861	-0.060447	4.815529
297.798283	8000.357733	12.243866	-0.060483	4.815481
298.059408	8000.431543	12.248871	-0.060532	4.815501
297.911956	8000.531713	12.253875	-0.060504	4.815531
298.109905	8000.219668	12.258880	-0.060541	4.815439
297.918627	8000.378970	12.263885	-0.060505	4.815487
297.779446	8000.399110	12.268890	-0.060480	4.815493
297.970221	8000.220560	12.273895	-0.060515	4.815440
297.759448	8000.418019	12.278899	-0.060476	4.815499
297.844294	8000.369188	12.283904	-0.060492	4.815484
297.895587	8000.445932	12.288909	-0.060501	4.815506
297.863532	8000.390886	12.293914	-0.060495	4.815490
297.987741	8000.203750	12.298919	-0.060518	4.815435
297.921346	8000.289231	12.303923	-0.060506	4.815460
297.822268	8000.258728	12.308928	-0.060487	4.815452
297.819266	8000.488493	12.313933	-0.060487	4.815519
297.861475	8000.458195	12.318938	-0.060495	4.815510
297.936708	8000.409204	12.323943	-0.060509	4.815495
297.878501	8000.512993	12.328947	-0.060498	4.815526
298.028555	8000.419280	12.333952	-0.060526	4.815498
298.154111	8000.213994	12.338957	-0.060549	4.815437
297.822818	8000.368837	12.343962	-0.060488	4.815484
298.072248	8000.468107	12.348967	-0.060534	4.815512
298.082138	8000.352829	12.353971	-0.060536	4.815478
298.085044	8000.234229	12.358976	-0.060536	4.815444
298.060306	8000.349261	12.363981	-0.060532	4.815477
298.087190	8000.393532	12.368986	-0.060537	4.815490
298.008456	8000.231891	12.373991	-0.060522	4.815443
297.936691	8000.384624	12.378995	-0.060509	4.815488
298.024756	8000.359362	12.384000	-0.060525	4.815480
297.886990	8000.401971	12.389005	-0.060500	4.815493
297.890641	8000.212837	12.394010	-0.060500	4.815438
297.964743	8000.359437	12.399015	-0.060514	4.815481
297.956288	8000.403122	12.404019	-0.060513	4.815493
297.827054	8000.388152	12.409024	-0.060489	4.815490
297.795314	8000.497724	12.414029	-0.060483	4.815522
298.010673	8000.361269	12.419034	-0.060523	4.815481
297.913620	8000.291250	12.424039	-0.060505	4.815461
297.744968	8000.520406	12.429043	-0.060473	4.815529
297.841850	8000.326403	12.434048	-0.060491	4.815472
297.796046	8000.419707	12.439053	-0.060483	4.815499
297.801205	8000.390933	12.444058	-0.060484	4.815491
297.946779	8000.154983	12.449063	-0.060511	4.815421
297.964675	8000.349820	12.454067	-0.060514	4.815478
298.048552	8000.188738	12.459072	-0.060530	4.815430
298.044284	8000.263490	12.464077	-0.060529	4.815452
298.054294	8000.308551	12.469082	-0.060531	4.815465
298.164383	8000.338168	12.474087	-0.060551	4.815473
298.064385	8000.226413	12.479091	-0.060533	4.815441
298.162944	8000.324249	12.484096	-0.060551	4.815469
298.151820	8000.269551	12.489101	-0.060549	4.815454
298.062114	8000.420918	12.494106	-0.060532	4.815498
298.161567	8000.240853	12.499111	-0.060551	4.815445
297.939106	8000.371846	12.504115	-0.060509	4.815484
297.927346	8000.184594	12.509120	-0.060507	4.815430
297.937218	8000.366471	12.514125	-0.060509	4.815483
298.095131	8000.347712	12.519130	-0.060539	4.815477
297.941209	8000.380434	12.524135	-0.060510	4.815487
297.979799	8000.425969	12.529139	-0.060517	4.815500
298.060035	8000.234897	12.534144	-0.060532	4.815444
298.196587	8000.353672	12.539149	-0.060557	4.815478
298.060119	8000.421958	12.544154	-0.060532	4.815498
298.034943	8000.272962	12.549159	-0.060527	4.815455
298.088776	8000.432054	12.554163	-0.060537	4.815501
298.248931	8000.221997	12.559168	-0.060567	4.815439
298.009641	8000.340954	12.564173	-0.060523	4.815475
297.939155	8000.300236	12.569178	-0.060509	4.815464
297.867330	8000.335388	12.574183	-0.060496	4.815474
297.855559	8000.353364	12.579187	-0.060494	4.815479
297.933059	8000.270207	12.584192	-0.060508	4.815455
298.057624	8000.333200	12.589197	-0.060532	4.815473
297.952985	8000.327190	12.594202	-0.060512	4.815471
297.909344	8000.521008	12.599207	-0.060504	4.815528
298.074323	8000.422198	12.604211	-0.060535	4.815498
298.137149	8000.205183	12.609216	-0.060546	4.815435
298.063699	8000.382473	12.614221	-0.060533	4.815487
298.110029	8000.365070	12.619226	-0.060541	4.815482
298.263171	8000.190171	12.624231	-0.060570	4.815430
298.043214	8000.301966	12.629235	-0.060529	4.815464
298.219079	8000.303814	12.634240	-0.060562	4.815463
298.303181	8000.377895	12.639245	-0.060577	4.815484
298.300549	8000.314786	12.644250	-0.060577	4.815466
298.159677	8000.361620	12.649255	-0.060551	4.815480
298.092922	8000.160628	12.654259	-0.060538	4.815422
298.156022	8000.277116	12.659264	-0.060550	4.815456
298.000613	8000.232853	12.664269	-0.060521	4.815444
297.980759	8000.247488	12.669274	-0.060517	4.815448
298.121195	8000.379155	12.674279	-0.060544	4.815486
298.000389	8000.276675	12.679283	-0.060521	4.815456
297.953204	8000.390266	12.684288	-0.060512	4.815490
297.919783	8000.478432	12.689293	-0.060506	4.815516
298.001939	8000.322665	12.694298	-0.060521	4.815470
298.150234	8000.267403	12.699303	-0.060549	4.815453
298.118976	8000.179235	12.704307	-0.060543	4.815427
298.274727	8000.247022	12.709312	-0.060572	4.815446
298.034826	8000.255871	12.714317	-0.060527	4.815450
298.102611	8000.171483	12.719322	-0.060540	4.815425
298.183446	8000.183513	12.724327	-0.060555	4.815428
298.075458	8000.415813	12.729331	-0.060535	4.815497
298.261589	8000.239323	12.734336	-0.060570	4.815444
298.362352	8000.538154	12.739341	-0.060589	4.815531
298.120794	8000.414428	12.744346	-0.060544	4.815496
297.955416	8000.374274	12.749351	-0.060513	4.815485
298.117854	8000.335281	12.754355	-0.060543	4.815473
298.217415	8000.333726	12.759360	-0.060562	4.815472
297.997380	8000.378178	12.764365	-0.060521	4.815486
298.113135	8000.256105	12.769370	-0.060542	4.815450
298.108194	8000.291297	12.774375	-0.060541	4.815460
298.007780	8000.313148	12.779379	-0.060522	4.815467
298.070247	8000.228672	12.784384	-0.060534	4.815442
298.226761	8000.385191	12.789389	-0.060563	4.815487
298.278072	8000.366802	12.794394	-0.060573	4.815481
298.370882	8000.213349	12.799399	-0.060590	4.815436
298.246012	8000.351306	12.804403	-0.060567	4.815477
298.186847	8000.115166	12.809408	-0.060556	4.815408
298.059387	8000.371728	12.814413	-0.060532	4.815484
298.061736	8000.404903	12.819418	-0.060533	4.815493
298.199242	8000.206229	12.824423	-0.060558	4.815435
297.950263	8000.555910	12.829427	-0.060512	4.815538
298.178739	8000.414328	12.834432	-0.060554	4.815496
298.278421	8000.445911	12.839437	-0.060573	4.815504
298.250688	8000.443314	12.844442	-0.060568	4.815504
298.095239	8000.238712	12.849447	-0.060539	4.815445
298.193027	8000.384636	12.854451	-0.060557	4.815487
298.073201	8000.376236	12.859456	-0.060535	4.815485
298.090741	8000.343391	12.864461	-0.060538	4.815475
298.151221	8000.250331	12.869466	-0.060549	4.815448
298.350181	8000.300663	12.874471	-0.060586	4.815462
298.209158	8000.405215	12.879475	-0.060560	4.815493
297.856507	8000.389747	12.884480	-0.060494	4.815490
297.996273	8000.458338	12.889485	-0.060521	4.815509
298.035219	8000.477156	12.894490	-0.060528	4.815515
298.071909	8000.294981	12.899495	-0.060535	4.815461
298.091918	8000.529405	12.904499	-0.060538	4.815530
298.393734	8000.235115	12.909504	-0.060594	4.815442
298.275110	8000.362486	12.914509	-0.060572	4.815480
298.240612	8000.534011	12.919514	-0.060566	4.815530
298.460330	8000.214842	12.924519	-0.060607	4.815436
298.331610	8000.390148	12.929523	-0.060583	4.815488
298.265136	8000.415768	12.934528	-0.060571	4.815496
298.268241	8000.405131	12.939533	-0.060571	4.815493
298.185653	8000.543790	12.944538	-0.060556	4.815533
298.203472	8000.258686	12.949543	-0.060559	4.815450
298.088018	8000.408557	12.954547	-0.060538	4.815494
298.294149	8000.363875	12.959552	-0.060576	4.815480
298.372259	8000.443202	12.964557	-0.060591	4.815503
298.089703	8000.386138	12.969562	-0.060538	4.815488
298.452913	8000.387888	12.974567	-0.060606	4.815487
298.331583	8000.427563	12.979571	-0.060583	4.815499
298.157879	8000.513403	12.984576	-0.060551	4.815525
298.310680	8000.428286	12.989581	-0.060579	4.815499
298.209634	8000.376372	12.994586	-0.060560	4.815484
298.302474	8000.304157	12.999591	-0.060578	4.815463
298.333508	8000.322843	13.004595	-0.060583	4.815468
298.434893	8000.287113	13.009600	-0.060602	4.815457
298.156809	8000.396875	13.014605	-0.060550	4.815491
298.107838	8000.414235	13.019610	-0.060541	4.815496
298.339054	8000.343246	13.024615	-0.060584	4.815474
298.276053	8000.446956	13.029619	-0.060573	4.815505
298.098318	8000.404458	13.034624	-0.060540	4.815493
298.036065	8000.234539	13.039629	-0.060528	4.815444
298.231878	8000.487912	13.044634	-0.060565	4.815517
298.364257	8000.264567	13.049639	-0.060589	4.815451
298.278555	8000.484411	13.054643	-0.060573	4.815516
298.156743	8000.557216	13.059648	-0.060551	4.815537
298.174809	8000.328767	13.064653	-0.060554	4.815471
298.111165	8000.466671	13.069658	-0.060542	4.815511
298.238076	8000.383263	13.074663	-0.060566	4.815486
298.373412	8000.407956	13.079667	-0.060591	4.815493
298.227423	8000.359571	13.084672	-0.060564	4.815479
298.152974	8000.305960	13.089677	-0.060550	4.815464
298.234535	8000.305175	13.094682	-0.060565	4.815464
298.409888	8000.296326	13.099687	-0.060598	4.815460
298.091842	8000.371220	13.104691	-0.060538	4.815483
298.246096	8000.507394	13.109696	-0.060567	4.815523
298.307425	8000.411139	13.114701	-0.060579	4.815494
298.001400	8000.390030	13.119706	-0.060522	4.815489
298.063616	8000.242484	13.124711	-0.060533	4.815446
297.995586	8000.376039	13.129715	-0.060521	4.815485
298.171826	8000.398203	13.134720	-0.060553	4.815491
298.155571	8000.349832	13.139725	-0.060550	4.815477
298.265432	8000.332414	13.144730	-0.060571	4.815471
298.265034	8000.431817	13.149735	-0.060571	4.815500
298.251216	8000.338593	13.154739	-0.060568	4.815473
298.227414	8000.493192	13.159744	-0.060564	4.815518
298.267130	8000.404061	13.164749	-0.060571	4.815492
298.047327	8000.494481	13.169754	-0.060530	4.815520
298.133352	8000.527976	13.174759	-0.060546	4.815529
298.122742	8000.506422	13.179763	-0.060544	4.815523
298.186739	8000.411281	13.184768	-0.060556	4.815495
298.293187	8000.418392	13.189773	-0.060576	4.815496
298.136113	8000.535505	13.194778	-0.060547	4.815531
298.294745	8000.386351	13.199783	-0.060576	4.815487
298.197763	8000.527978	13.204787	-0.060558	4.815529
298.211527	8000.413832	13.209792	-0.060561	4.815495
298.320138	8000.491527	13.214797	-0.060581	4.815518
298.375176	8000.433650	13.219802	-0.060591	4.815500
298.223469	8000.439685	13.224807	-0.060563	4.815503
298.221657	8000.516618	13.229811	-0.060563	4.815525
298.287765	8000.551921	13.234816	-0.060575	4.815535
298.179272	8000.427195	13.239821	-0.060555	4.815499
298.225209	8000.544470	13.244826	-0.060564	4.815533
298.426889	8000.416338	13.249831	-0.060601	4.815495
298.319406	8000.332249	13.254835	-0.060581	4.815471
298.229876	8000.410933	13.259840	-0.060564	4.815494
298.304258	8000.327723	13.264845	-0.060578	4.815470
298.045429	8000.535076	13.269850	-0.060530	4.815532
298.134078	8000.410414	13.274855	-0.060546	4.815495
298.115039	8000.543714	13.279859	-0.060543	4.815534
298.360045	8000.402405	13.284864	-0.060589	4.815491
298.291708	8000.518854	13.289869	-0.060576	4.815526
298.192545	8000.400697	13.294874	-0.060557	4.815492
298.455840	8000.498061	13.299879	-0.060606	4.815519
298.201681	8000.508810	13.304883	-0.060559	4.815523
298.121686	8000.460451	13.309888	-0.060544	4.815509
298.179011	8000.430403	13.314893	-0.060555	4.815500
298.031679	8000.473923	13.319898	-0.060527	4.815514
298.190461	8000.386769	13.324903	-0.060557	4.815488
298.068656	8000.577154	13.329907	-0.060534	4.815544
298.437981	8000.336360	13.334912	-0.060603	4.815472
298.394983	8000.398713	13.339917	-0.060595	4.815490
298.175666	8000.432488	13.344922	-0.060554	4.815501
298.349196	8000.390472	13.349927	-0.060587	4.815488
298.188530	8000.628315	13.354931	-0.060557	4.815558
298.187103	8000.542778	13.359936	-0.060557	4.815533
298.207008	8000.433010	13.364941	-0.060560	4.815501
298.496979	8000.543644	13.369946	-0.060614	4.815532
298.436767	8000.427201	13.374951	-0.060603	4.815498
298.324666	8000.502305	13.379955	-0.060582	4.815521
298.348271	8000.263259	13.384960	-0.060586	4.815451
298.323776	8000.376158	13.389965	-0.060582	4.815484
298.210317	8000.450169	13.394970	-0.060561	4.815506
298.362673	8000.380011	13.399975	-0.060589	4.815485
298.229985	8000.513563	13.404979	-0.060565	4.815524
298.317866	8000.540676	13.409984	-0.060581	4.815532
298.395120	8000.528062	13.414989	-0.060595	4.815528
298.372043	8000.535162	13.419994	-0.060591	4.815530
298.382030	8000.264891	13.424999	-0.060593	4.815451
298.477670	8000.380852	13.430003	-0.060611	4.815484
298.220206	8000.392615	13.435008	-0.060563	4.815489
298.291269	8000.202459	13.440013	-0.060576	4.815433
298.474885	8000.153128	13.445018	-0.060610	4.815418
298.307079	8000.163173	13.450023	-0.060579	4.815422
298.268359	8000.388071	13.455027	-0.060572	4.815488
298.319389	8000.397469	13.460032	-0.060581	4.815490
298.374813	8000.289359	13.465037	-0.060591	4.815458
298.411484	8000.374412	13.470042	-0.060598	4.815483
298.465654	8000.399896	13.475047	-0.060608	4.815490
298.355383	8000.363862	13.480051	-0.060588	4.815480
298.298639	8000.386438	13.485056	-0.060577	4.815487
298.407471	8000.258904	13.490061	-0.060597	4.815449
298.259402	8000.535436	13.495066	-0.060570	4.815531
298.450177	8000.222201	13.500071	-0.060605	4.815438
298.550641	8000.389550	13.505075	-0.060624	4.815487
298.275476	8000.353988	13.510080	-0.060573	4.815478
298.238425	8000.281757	13.515085	-0.060566	4.815457
298.228117	8000.607607	13.520090	-0.060564	4.815552
298.257505	8000.385758	13.525095	-0.060570	4.815487
298.341599	8000.432048	13.530099	-0.060585	4.815500
298.197628	8000.525863	13.535104	-0.060559	4.815528
298.357940	8000.413080	13.540109	-0.060588	4.815494
298.242950	8000.542650	13.545114	-0.060567	4.815533
298.571565	8000.450830	13.550119	-0.060628	4.815504
298.641569	8000.376098	13.555123	-0.060641	4.815482
298.475533	8000.516580	13.560128	-0.060610	4.815524
298.541896	8000.404375	13.565133	-0.060623	4.815491
298.483491	8000.452577	13.570138	-0.060612	4.815505
298.646157	8000.266076	13.575143	-0.060642	4.815450
298.476745	8000.375503	13.580147	-0.060611	4.815483
298.365261	8000.438859	13.585152	-0.060590	4.815502
298.542994	8000.401188	13.590157	-0.060623	4.815490
298.463576	8000.405216	13.595162	-0.060608	4.815492
298.652652	8000.382699	13.600167	-0.060643	4.815484
298.575677	8000.429524	13.605171	-0.060629	4.815498
298.409502	8000.422492	13.610176	-0.060598	4.815497
298.608510	8000.406553	13.615181	-0.060635	4.815491
298.497128	8000.388672	13.620186	-0.060614	4.815487
298.596805	8000.294123	13.625191	-0.060633	4.815459
298.364244	8000.481602	13.630195	-0.060590	4.815514
298.536667	8000.396811	13.635200	-0.060622	4.815489
298.684412	8000.319093	13.640205	-0.060649	4.815465
298.422626	8000.517847	13.645210	-0.060601	4.815525
298.583132	8000.267175	13.650215	-0.060630	4.815451
298.291498	8000.521017	13.655219	-0.060576	4.815526
298.360012	8000.520016	13.660224	-0.060589	4.815526
298.545952	8000.413001	13.665229	-0.060624	4.815493
298.450542	8000.434935	13.670234	-0.060606	4.815500
298.424913	8000.385340	13.675239	-0.060601	4.815486
298.322112	8000.520457	13.680243	-0.060582	4.815526
298.490130	8000.369320	13.685248	-0.060613	4.815481
298.487094	8000.414165	13.690253	-0.060613	4.815494
298.312277	8000.518158	13.695258	-0.060580	4.815525
298.651989	8000.362386	13.700263	-0.060643	4.815478
298.693371	8000.418657	13.705267	-0.060651	4.815494
298.399663	8000.538849	13.710272	-0.060596	4.815531
298.299571	8000.438848	13.715277	-0.060578	4.815502
298.460138	8000.485338	13.720282	-0.060608	4.815515
298.525763	8000.419085	13.725287	-0.060620	4.815495
298.583230	8000.378350	13.730291	-0.060630	4.815483
298.459292	8000.429741	13.735296	-0.060607	4.815499
298.554224	8000.403524	13.740301	-0.060625	4.815491
298.413041	8000.524109	13.745306	-0.060599	4.815527
298.552781	8000.420604	13.750311	-0.060625	4.815496
298.275704	8000.489764	13.755315	-0.060573	4.815517
298.448531	8000.431702	13.760320	-0.060605	4.815499
298.689623	8000.420737	13.765325	-0.060650	4.815495
298.640753	8000.588819	13.770330	-0.060641	4.815544
298.611629	8000.340344	13.775335	-0.060636	4.815472
298.529665	8000.502530	13.780339	-0.060621	4.815520
298.477076	8000.550829	13.785344	-0.060611	4.815534
298.637620	8000.394222	13.790349	-0.060641	4.815488
298.506074	8000.538484	13.795354	-0.060616	4.815530
298.594434	8000.376404	13.800359	-0.060633	4.815483
298.703812	8000.511835	13.805363	-0.060653	4.815522
298.611351	8000.514577	13.810368	-0.060636	4.815523
298.594943	8000.375345	13.815373	-0.060633	4.815482
298.606304	8000.550838	13.820378	-0.060635	4.815533
298.633200	8000.285122	13.825383	-0.060640	4.815456
298.494419	8000.385436	13.830387	-0.060614	4.815486
298.431677	8000.550080	13.835392	-0.060602	4.815534
298.582958	8000.405078	13.840397	-0.060631	4.815491
298.588447	8000.499235	13.845402	-0.060632	4.815518
298.680696	8000.416320	13.850407	-0.060649	4.815494
298.568146	8000.492485	13.855411	-0.060628	4.815517
298.642518	8000.412481	13.860416	-0.060642	4.815493
298.638568	8000.411347	13.865421	-0.060641	4.815493
298.761037	8000.511721	13.870426	-0.060664	4.815521
298.803041	8000.413007	13.875431	-0.060672	4.815492
298.510908	8000.509709	13.880435	-0.060617	4.815522
298.447432	8000.539656	13.885440	-0.060605	4.815531
298.617437	8000.539270	13.890445	-0.060637	4.815530
298.524490	8000.538797	13.895450	-0.060620	4.815530
298.445074	8000.429518	13.900455	-0.060605	4.815499
298.674543	8000.543426	13.905459	-0.060648	4.815531
298.774564	8000.432847	13.910464	-0.060666	4.815498
298.673002	8000.416198	13.915469	-0.060647	4.815494
298.389289	8000.412560	13.920474	-0.060595	4.815494
298.525504	8000.410545	13.925479	-0.060620	4.815493
298.557306	8000.644100	13.930483	-0.060626	4.815561
298.659005	8000.496137	13.935488	-0.060645	4.815517
298.727867	8000.455591	13.940493	-0.060658	4.815505
298.647315	8000.529081	13.945498	-0.060643	4.815527
298.726694	8000.530398	13.950503	-0.060658	4.815527
298.733335	8000.489889	13.955507	-0.060659	4.815515
298.808718	8000.547794	13.960512	-0.060673	4.815532
298.749841	8000.401442	13.965517	-0.060662	4.815489
298.558768	8000.531889	13.970522	-0.060626	4.815528
298.677678	8000.556310	13.975527	-0.060648	4.815535
298.595632	8000.510054	13.980531	-0.060633	4.815522
298.520992	8000.525919	13.985536	-0.060619	4.815527
298.653756	8000.446883	13.990541	-0.060644	4.815503
298.614228	8000.618326	13.995546	-0.060637	4.815553
298.667747	8000.410773	14.000551	-0.060646	4.815492
298.485064	8000.516773	14.005555	-0.060613	4.815524
298.744696	8000.523219	14.010560	-0.060661	4.815525
298.557092	8000.343734	14.015565	-0.060626	4.815473
298.600349	8000.537928	14.020570	-0.060634	4.815530
298.784429	8000.318645	14.025575	-0.060668	4.815465
298.654713	8000.411628	14.030579	-0.060644	4.815493
298.532560	8000.514356	14.035584	-0.060621	4.815523
298.648824	8000.299294	14.040589	-0.060643	4.815460
298.470344	8000.529359	14.045594	-0.060610	4.815528
298.436463	8000.539487	14.050599	-0.060604	4.815531
298.476950	8000.409749	14.055603	-0.060611	4.815493
298.460191	8000.505675	14.060608	-0.060608	4.815521
298.666512	8000.526202	14.065613	-0.060646	4.815526
298.458684	8000.548408	14.070618	-0.060608	4.815533
298.814821	8000.407874	14.075623	-0.060674	4.815491
298.752580	8000.541527	14.080627	-0.060662	4.815530
298.640816	8000.535397	14.085632	-0.060642	4.815529
298.709230	8000.406123	14.090637	-0.060654	4.815491
298.621189	8000.628070	14.095642	-0.060638	4.815556
298.481828	8000.392731	14.100647	-0.060612	4.815488
298.475319	8000.449277	14.105651	-0.060611	4.815504
298.675835	8000.481465	14.110656	-0.060648	4.815513
298.680430	8000.359683	14.115661	-0.060649	4.815477
298.638334	8000.538566	14.120666	-0.060641	4.815530
298.553418	8000.436678	14.125671	-0.060625	4.815500
298.566669	8000.439036	14.130675	-0.060628	4.815501
298.415359	8000.556246	14.135680	-0.060600	4.815536
298.694881	8000.538437	14.140685	-0.060652	4.815529
298.707784	8000.445654	14.145690	-0.060654	4.815502
298.597516	8000.386103	14.150695	-0.060634	4.815485
298.545822	8000.538102	14.155699	-0.060624	4.815530
298.610062	8000.433344	14.160704	-0.060636	4.815499
298.754211	8000.387635	14.165709	-0.060663	4.815485
298.572603	8000.546030	14.170714	-0.060629	4.815532
298.575516	8000.290606	14.175719	-0.060629	4.815458
298.738441	8000.531680	14.180723	-0.060660	4.815527
298.696210	8000.397363	14.185728	-0.060652	4.815488
298.762589	8000.550254	14.190733	-0.060664	4.815532
298.772456	8000.508729	14.195738	-0.060666	4.815520
298.847486	8000.397736	14.200743	-0.060680	4.815488
298.770317	8000.530073	14.205747	-0.060666	4.815527
298.850931	8000.530342	14.210752	-0.060681	4.815526
298.865525	8000.523102	14.215757	-0.060684	4.815524
298.810114	8000.524321	14.220762	-0.060673	4.815525
298.777475	8000.269374	14.225767	-0.060667	4.815450
298.599287	8000.543271	14.230771	-0.060634	4.815531
298.736572	8000.519895	14.235776	-0.060660	4.815524
298.727353	8000.355127	14.240781	-0.060658	4.815476
298.660203	8000.551766	14.245786	-0.060645	4.815533
298.823449	8000.446512	14.250791	-0.060676	4.815502
298.606965	8000.591503	14.255795	-0.060636	4.815545
298.702801	7999.453642	14.260800	-0.060653	4.815212
298.853954	7996.246641	14.265805	-0.060679	4.814275
298.640687	7990.659274	14.270810	-0.060635	4.812643
298.690803	7983.946166	14.275815	-0.060640	4.810681
298.823277	7976.689528	14.280819	-0.060660	4.808558
298.644614	7969.015038	14.285824	-0.060622	4.806314
298.622154	7961.278400	14.290829	-0.060613	4.804049
298.675586	7953.318504	14.295834	-0.060618	4.801718
298.629576	7945.401427	14.300839	-0.060604	4.799399
298.454682	7937.436215	14.305843	-0.060566	4.797065
298.381293	7929.414735	14.310848	-0.060547	4.794713
298.518504	7921.410956	14.315853	-0.060567	4.792364
298.344793	7913.347013	14.320858	-0.060530	4.789997
298.329742	7905.372289	14.325863	-0.060522	4.787655
298.464543	7897.398284	14.330867	-0.060542	4.785312
298.399476	7889.372280	14.335872	-0.060524	4.782952
298.293686	7881.453704	14.340877	-0.060500	4.780624
298.129209	7873.393996	14.345882	-0.060464	4.778252
298.247858	7865.401498	14.350887	-0.060481	4.775899
297.947959	7857.365025	14.355891	-0.060420	4.773533
297.891476	7849.311451	14.360896	-0.060404	4.771159
298.140307	7841.370597	14.365901	-0.060445	4.768817
298.097248	7833.359011	14.370906	-0.060432	4.766453
298.113359	7825.373303	14.375911	-0.060430	4.764096
298.150473	7817.389692	14.380915	-0.060431	4.761739
297.995703	7809.341179	14.385920	-0.060397	4.759361
297.849296	7801.433064	14.390925	-0.060365	4.757024
297.860139	7793.328090	14.395930	-0.060362	4.754627
297.995712	7785.305630	14.400935	-0.060382	4.752253
297.782818	7777.306432	14.405939	-0.060337	4.749885
297.930223	7769.361639	14.410944	-0.060359	4.747532
298.041489	7761.292905	14.415949	-0.060374	4.745140
297.882444	7753.365350	14.420954	-0.060340	4.742790
297.648662	7745.308438	14.425959	-0.060291	4.740401
297.759775	7737.350705	14.430963	-0.060306	4.738039
297.773894	7729.320252	14.435968	-0.060304	4.735654
297.585764	7721.304466	14.440973	-0.060264	4.733273
297.392594	7713.313747	14.445978	-0.060222	4.730899
297.487790	7705.307806	14.450983	-0.060235	4.728518
297.411493	7697.286450	14.455987	-0.060215	4.726131
297.418400	7689.265743	14.460992	-0.060211	4.723743
297.487803	7681.346062	14.465997	-0.060219	4.721384
297.223597	7673.283933	14.471002	-0.060165	4.718983
297.356053	7665.343490	14.476007	-0.060184	4.716615
297.287251	7657.321617	14.481011	-0.060166	4.714222
297.577258	7649.293158	14.486016	-0.060215	4.711825
297.488388	7641.308548	14.491021	-0.060193	4.709442
297.295982	7633.316778	14.496026	-0.060152	4.707054
297.138170	7625.306431	14.501031	-0.060118	4.704660
297.192779	7617.287172	14.506035	-0.060123	4.702262
297.291754	7609.249359	14.511040	-0.060136	4.699857
297.536500	7601.375121	14.516045	-0.060176	4.697499
297.487849	7593.299565	14.521050	-0.060162	4.695081
297.241888	7585.264403	14.526055	-0.060111	4.692673
297.319074	7577.254257	14.531059	-0.060120	4.690271
297.474748	7569.267404	14.536064	-0.060144	4.687875
297.427232	7561.249054	14.541069	-0.060130	4.685469
297.121833	7553.301966	14.546074	-0.060068	4.683083
297.033272	7545.304161	14.551079	-0.060046	4.680680
297.014546	7537.308805	14.556083	-0.060037	4.678277
296.873991	7529.255710	14.561088	-0.060006	4.675855
297.012767	7521.253884	14.566093	-0.060027	4.673447
296.838222	7513.136448	14.571098	-0.059989	4.671004
296.719496	7505.179020	14.576103	-0.059961	4.668607
296.778175	7497.224443	14.581107	-0.059967	4.666210
296.759173	7489.203225	14.586112	-0.059958	4.663791
297.023857	7481.239053	14.591117	-0.060003	4.661388
296.598489	7473.226620	14.596122	-0.059918	4.658970
296.779267	7465.222788	14.601127	-0.059947	4.656553
297.063785	7457.235803	14.606131	-0.059994	4.654139
296.649007	7449.169029	14.611136	-0.059912	4.651701
296.529950	7441.201457	14.616141	-0.059885	4.649291
296.546671	7433.220926	14.621146	-0.059882	4.646876
296.449822	7425.195795	14.626151	-0.059859	4.644446
296.449162	7417.241085	14.631155	-0.059854	4.642036
296.433958	7409.197805	14.636160	-0.059846	4.639598
296.319247	7401.298530	14.641165	-0.059819	4.637202
296.168942	7393.201707	14.646170	-0.059786	4.634746
296.314457	7385.175542	14.651175	-0.059808	4.632309
296.286533	7377.158431	14.656179	-0.059798	4.629874
296.349051	7369.177513	14.661184	-0.059804	4.627448
296.410903	7361.177154	14.666189	-0.059810	4.625016
296.201943	7353.169454	14.671194	-0.059766	4.622580
296.158490	7345.157983	14.676199	-0.059753	4.620141
296.238106	7337.224620	14.681203	-0.059762	4.617725
296.191807	7329.158088	14.686208	-0.059749	4.615267
296.196680	7321.209524	14.691213	-0.059744	4.612844
296.128290	7313.092223	14.696218	-0.059726	4.610368
296.049102	7305.163401	14.701223	-0.059706	4.607948
296.254221	7297.136445	14.706227	-0.059739	4.605497
296.192038	7289.177199	14.711232	-0.059723	4.603065
296.073921	7281.180374	14.716237	-0.059695	4.600620
295.950728	7273.159285	14.721242	-0.059667	4.598167
296.181183	7265.176783	14.726247	-0.059705	4.595724
296.000754	7257.146012	14.731251	-0.059666	4.593266
295.782492	7249.078927	14.736256	-0.059620	4.590794
295.883581	7241.148085	14.741261	-0.059634	4.588363
295.765996	7233.096666	14.746266	-0.059607	4.585894
295.787910	7225.129692	14.751271	-0.059606	4.583450
295.774913	7217.129435	14.756275	-0.059598	4.580994
295.542661	7209.077142	14.761280	-0.059550	4.578520
295.637013	7201.140110	14.766285	-0.059562	4.576081
295.546107	7193.101251	14.771290	-0.059540	4.573609
295.501793	7185.111273	14.776295	-0.059526	4.571151
295.415596	7177.111563	14.781299	-0.059505	4.568688
295.451468	7169.086389	14.786304	-0.059507	4.566216
295.554137	7161.175704	14.791309	-0.059521	4.563779
295.440832	7153.114169	14.796314	-0.059494	4.561293
295.502703	7145.138310	14.801319	-0.059500	4.558832
295.403994	7137.165411	14.806323	-0.059477	4.556371
295.379690	7129.124777	14.811328	-0.059467	4.553888
295.304631	7121.071614	14.816333	-0.059448	4.551400
295.312616	7113.049743	14.821338	-0.059444	4.548919
295.255780	7105.097157	14.826343	-0.059428	4.546459
295.278152	7097.126302	14.831347	-0.059427	4.543992
295.281988	7089.107468	14.836352	-0.059423	4.541509
295.449692	7081.126346	14.841357	-0.059449	4.539036
295.289967	7073.153449	14.846362	-0.059414	4.536564
295.057219	7065.100888	14.851367	-0.059365	4.534066
295.083477	7057.112591	14.856371	-0.059365	4.531587
294.973465	7049.068231	14.861376	-0.059339	4.529089
294.987262	7041.114934	14.866381	-0.059337	4.526618
294.898540	7033.058252	14.871386	-0.059315	4.524113
294.869161	7025.120050	14.876391	-0.059304	4.521644
294.772149	7017.111476	14.881395	-0.059281	4.519151
294.901006	7009.106694	14.886400	-0.059300	4.516659
294.909193	7001.072144	14.891405	-0.059296	4.514156
294.705279	6992.999657	14.896410	-0.059253	4.511639
294.752333	6985.035827	14.901415	-0.059257	4.509155
294.910818	6977.031457	14.906419	-0.059281	4.506657
294.933457	6969.014618	14.911424	-0.059280	4.504154
294.855344	6961.093009	14.916429	-0.059260	4.501679
294.760547	6953.080090	14.921434	-0.059237	4.499174
294.880205	6945.053792	14.926439	-0.059254	4.496664
294.734939	6937.044335	14.931443	-0.059222	4.494157
294.532958	6929.011037	14.936448	-0.059179	4.491641
294.409758	6921.044337	14.941453	-0.059151	4.489144
294.372735	6913.037478	14.946458	-0.059139	4.486634
294.239292	6905.003242	14.951463	-0.059109	4.484114
294.402253	6897.075008	14.956467	-0.059134	4.481626
294.367150	6889.020965	14.961472	-0.059122	4.479097
294.309222	6881.125712	14.966477	-0.059106	4.476616
294.419640	6872.999743	14.971482	-0.059122	4.474062
294.173171	6865.027143	14.976487	-0.059071	4.471554
294.261206	6856.993924	14.981491	-0.059082	4.469026
294.007128	6849.024591	14.986496	-0.059029	4.466515
294.059477	6840.999864	14.991501	-0.059034	4.463987
294.055488	6833.030820	14.996506	-0.059028	4.461475
293.979390	6824.975110	15.001511	-0.059008	4.458934
294.085618	6817.058300	15.006515	-0.059023	4.456435
294.122544	6809.016283	15.011520	-0.059025	4.453896
293.956546	6801.016932	15.016525	-0.058989	4.451368
293.817715	6793.010010	15.021530	-0.058957	4.448836
293.929681	6784.980810	15.026535	-0.058973	4.446296
294.027472	6777.019455	15.031539	-0.058986	4.443777
293.740410	6769.020369	15.036544	-0.058927	4.441242
293.940755	6761.040115	15.041549	-0.058960	4.438715
293.902861	6753.012452	15.046554	-0.058947	4.436169
293.677278	6744.963480	15.051559	-0.058900	4.433615
293.828835	6736.932646	15.056563	-0.058923	4.431066
293.615956	6728.966585	15.061568	-0.058878	4.428535
293.729034	6720.956284	15.066573	-0.058894	4.425990
293.672118	6712.981498	15.071578	-0.058878	4.423454
293.583352	6704.959794	15.076583	-0.058856	4.420902
293.717450	6696.984530	15.081587	-0.058876	4.418363
293.685695	6688.932049	15.086592	-0.058865	4.415798
293.766697	6680.984384	15.091597	-0.058875	4.413266
293.591631	6672.948344	15.096602	-0.058837	4.410702
293.472063	6664.962153	15.101607	-0.058810	4.408154
293.490632	6656.940309	15.106611	-0.058808	4.405593
293.480907	6648.955829	15.111616	-0.058801	4.403042
293.457612	6641.008431	15.116621	-0.058791	4.400502
293.312191	6633.043260	15.121626	-0.058759	4.397953
293.649434	6624.977174	15.126631	-0.058817	4.395374
293.565304	6616.955961	15.131635	-0.058796	4.392805
293.388692	6608.905018	15.136640	-0.058758	4.390225
293.496315	6600.986382	15.141645	-0.058773	4.387687
293.293174	6592.932743	15.146650	-0.058729	4.385103
293.167265	6584.969126	15.151655	-0.058701	4.382546
293.194343	6576.993872	15.156659	-0.058701	4.379985
293.110575	6568.996143	15.161664	-0.058680	4.377415
293.296373	6560.995319	15.166669	-0.058709	4.374843
293.108346	6552.979836	15.171674	-0.058669	4.372264
293.372521	6544.914193	15.176679	-0.058713	4.369669
293.239297	6537.041940	15.181683	-0.058683	4.367133
292.993515	6528.955654	15.186688	-0.058632	4.364525
293.067104	6521.007540	15.191693	-0.058641	4.361963
293.032182	6512.983961	15.196698	-0.058629	4.359374
292.937102	6505.022422	15.201703	-0.058606	4.356803
292.894645	6496.966038	15.206707	-0.058593	4.354200
293.019551	6488.817487	15.211712	-0.058611	4.351567
293.107480	6480.874327	15.216717	-0.058622	4.348998
292.914592	6472.907804	15.221722	-0.058581	4.346419
292.867308	6464.905507	15.226727	-0.058567	4.343827
292.951181	6456.953451	15.231731	-0.058577	4.341251
292.814795	6448.951984	15.236736	-0.058547	4.338656
292.679474	6440.997677	15.241741	-0.058516	4.336075
292.578367	6432.916669	15.246746	-0.058492	4.333451
292.468007	6424.904226	15.251751	-0.058466	4.330848
292.548463	6416.940522	15.256755	-0.058476	4.328261
292.575315	6408.917465	15.261760	-0.058476	4.325652
292.404206	6400.978446	15.266765	-0.058439	4.323067
292.366910	6392.952110	15.271770	-0.058427	4.320454
292.334143	6384.956419	15.276775	-0.058416	4.317849
292.349586	6376.959692	15.281779	-0.058413	4.315242
292.386158	6368.884064	15.286784	-0.058415	4.312609
292.555661	6360.882971	15.291789	-0.058441	4.309999
292.522876	6352.915271	15.296794	-0.058430	4.307397
292.286008	6344.901801	15.301799	-0.058380	4.304776
292.428462	6336.949241	15.306803	-0.058402	4.302177
292.080089	6328.914896	15.311808	-0.058332	4.299546
292.127279	6320.941880	15.316813	-0.058335	4.296936
292.040812	6312.936922	15.321818	-0.058314	4.294313
291.894645	6304.900268	15.326823	-0.058282	4.291678
291.973159	6296.892579	15.331827	-0.058291	4.289053
291.917443	6288.896909	15.336832	-0.058275	4.286428
291.803802	6280.923774	15.341837	-0.058249	4.283809
291.853139	6272.921060	15.346842	-0.058253	4.281180
291.937254	6264.922366	15.351847	-0.058263	4.278551
291.934998	6256.922237	15.356851	-0.058258	4.275919
291.950711	6248.878223	15.361856	-0.058256	4.273272
291.880084	6240.853760	15.366861	-0.058237	4.270628
291.763726	6232.885689	15.371866	-0.058210	4.268001
291.795722	6224.859988	15.376871	-0.058211	4.265354
291.883166	6216.898319	15.381875	-0.058222	4.262728
291.513051	6208.878168	15.386880	-0.058148	4.260076
291.497903	6200.915937	15.391885	-0.058140	4.257445
291.540242	6192.884389	15.396890	-0.058143	4.254790
291.328321	6184.846879	15.401895	-0.058098	4.252129
291.404405	6176.904610	15.406899	-0.058107	4.249501
291.443468	6168.903245	15.411904	-0.058109	4.246851
291.611641	6160.915500	15.416909	-0.058135	4.244205
291.510518	6152.906374	15.421914	-0.058111	4.241548
291.205645	6144.883636	15.426919	-0.058049	4.238883
291.373431	6136.969138	15.431923	-0.058075	4.236256
291.177487	6128.895225	15.436928	-0.058033	4.233571
291.145352	6120.868720	15.441933	-0.058022	4.230902
291.244198	6112.890393	15.446938	-0.058035	4.228249
291.366041	6104.853554	15.451943	-0.058053	4.225575
291.414257	6096.976653	15.456947	-0.058057	4.222951
291.269971	6088.889372	15.461952	-0.058025	4.220254
291.289701	6080.932494	15.466957	-0.058023	4.217601
291.164308	6072.888668	15.471962	-0.057994	4.214915
291.153308	6064.894228	15.476967	-0.057987	4.212245
291.116204	6056.865504	15.481971	-0.057975	4.209561
291.064626	6048.922635	15.486976	-0.057960	4.206905
290.983687	6040.917625	15.491981	-0.057940	4.204226
290.814548	6032.984815	15.496986	-0.057903	4.201568
290.796108	6024.937812	15.501991	-0.057895	4.198872
290.703377	6016.963495	15.506995	-0.057872	4.196197
290.686250	6008.870968	15.512000	-0.057864	4.193482
290.693727	6000.836840	15.517005	-0.057860	4.190786
290.431816	5992.845316	15.522010	-0.057806	4.188099
290.379610	5984.842068	15.527015	-0.057791	4.185408
290.513500	5976.896427	15.532019	-0.057811	4.182737
290.511194	5968.858243	15.537024	-0.057805	4.180032
290.686961	5960.946401	15.542029	-0.057833	4.177370
290.765521	5952.895481	15.547034	-0.057842	4.174657
290.474641	5944.887014	15.552039	-0.057783	4.171954
290.565110	5936.876692	15.557043	-0.057794	4.169252
290.480293	5928.857078	15.562048	-0.057773	4.166543
290.539430	5920.891442	15.567053	-0.057779	4.163853
290.441778	5912.915951	15.572058	-0.057756	4.161155
290.330933	5904.900000	15.577063	-0.057730	4.158442
290.355811	5896.924318	15.582067	-0.057729	4.155743
290.301027	5888.864431	15.587072	-0.057714	4.153012
290.241721	5880.861594	15.592077	-0.057698	4.150299
290.210520	5872.867642	15.597082	-0.057687	4.147587
290.181803	5864.822759	15.602087	-0.057676	4.144856
290.183102	5856.899762	15.607091	-0.057671	4.142165
290.087307	5848.850371	15.612096	-0.057648	4.139428
290.221167	5840.905528	15.617101	-0.057668	4.136728
290.163464	5832.856224	15.622106	-0.057652	4.133988
290.065263	5824.835745	15.627111	-0.057628	4.131256
290.062660	5816.882182	15.632115	-0.057623	4.128546
290.006266	5808.840620	15.637120	-0.057607	4.125803
289.993206	5800.910782	15.642125	-0.057599	4.123097
289.897354	5792.907858	15.647130	-0.057576	4.120364
289.975197	5784.919387	15.652135	-0.057586	4.117635
289.951281	5776.895245	15.657139	-0.057576	4.114892
289.753349	5768.805443	15.662144	-0.057534	4.112122
290.025420	5760.796486	15.667149	-0.057579	4.109383
289.847371	5752.864448	15.672154	-0.057541	4.106664
289.684158	5744.855242	15.677159	-0.057505	4.103916
289.864189	5736.900229	15.682163	-0.057534	4.101190
289.700629	5728.915444	15.687168	-0.057498	4.098447
289.527779	5720.920083	15.692173	-0.057461	4.095698
289.661190	5712.916473	15.697178	-0.057480	4.092949
289.663730	5704.863408	15.702183	-0.057475	4.090179
289.478090	5696.922013	15.707187	-0.057436	4.087443
289.361413	5688.865505	15.712192	-0.057409	4.084667
289.445899	5680.940590	15.717197	-0.057419	4.081936
289.669458	5672.922215	15.722202	-0.057456	4.079174
289.571033	5664.935612	15.727207	-0.057432	4.076416
289.742762	5656.897530	15.732211	-0.057459	4.073643
289.571733	5648.853396	15.737216	-0.057422	4.070861
289.415121	5640.889160	15.742221	-0.057387	4.068104
289.430947	5632.880084	15.747226	-0.057385	4.065333
289.473077	5624.945691	15.752231	-0.057388	4.062586
289.511098	5616.927661	15.757235	-0.057390	4.059808
289.169096	5608.966806	15.762240	-0.057321	4.057042
289.135342	5600.931284	15.767245	-0.057309	4.054253
289.229411	5592.932833	15.772250	-0.057322	4.051477
288.864247	5584.920446	15.777255	-0.057248	4.048688
289.019743	5576.916963	15.782259	-0.057272	4.045907
288.988195	5568.954636	15.787264	-0.057261	4.043136
288.907762	5560.917406	15.792269	-0.057241	4.040336
288.923578	5552.933631	15.797274	-0.057239	4.037554
288.851153	5544.921547	15.802279	-0.057220	4.034760
288.790862	5536.833139	15.807283	-0.057203	4.031936
288.520106	5528.831032	15.812288	-0.057148	4.029138
288.527542	5520.853782	15.817293	-0.057144	4.026351
288.762220	5512.884643	15.822298	-0.057183	4.023568
288.574973	5504.908197	15.827303	-0.057143	4.020774
288.501031	5496.925263	15.832307	-0.057124	4.017978
288.566225	5488.875865	15.837312	-0.057130	4.015158
288.566145	5480.890181	15.842317	-0.057125	4.012358
288.433551	5472.867960	15.847322	-0.057095	4.009541
288.418575	5464.909276	15.852327	-0.057087	4.006746
288.466013	5456.917824	15.857331	-0.057091	4.003939
288.494258	5448.900879	15.862336	-0.057091	4.001120
288.414714	5440.916642	15.867341	-0.057071	3.998310
288.578308	5432.889757	15.872346	-0.057096	3.995486
288.365554	5424.843194	15.877351	-0.057051	3.992647
288.395902	5416.869163	15.882355	-0.057052	3.989835
288.497179	5408.892167	15.887360	-0.057065	3.987022
288.204225	5400.900147	15.892365	-0.057006	3.984195
288.166335	5392.916191	15.897370	-0.056993	3.981373
288.236857	5384.916086	15.902375	-0.057001	3.978545
288.419207	5376.934921	15.907379	-0.057030	3.975724
287.899692	5368.912219	15.912384	-0.056928	3.972874
288.001932	5360.899553	15.917389	-0.056942	3.970036
288.095619	5352.913226	15.922394	-0.056954	3.967206
287.909970	5344.884333	15.927399	-0.056914	3.964353
287.901206	5336.984646	15.932403	-0.056908	3.961547
287.869601	5328.956434	15.937408	-0.056897	3.958693
288.015434	5320.966708	15.942413	-0.056919	3.955854
287.868668	5312.944232	15.947418	-0.056886	3.952996
288.005205	5304.870909	15.952423	-0.056906	3.950123
288.041026	5296.912522	15.957427	-0.056908	3.947287
287.866090	5288.914187	15.962432	-0.056870	3.944431
287.895271	5280.966757	15.967437	-0.056870	3.941595
287.761729	5272.968433	15.972442	-0.056840	3.938735
287.839741	5264.961991	15.977447	-0.056849	3.935875
287.830379	5257.008444	15.982451	-0.056842	3.933029
287.798299	5248.921445	15.987456	-0.056831	3.930134
287.723670	5240.954938	15.992461	-0.056812	3.927278
287.677220	5232.946708	15.997466	-0.056798	3.924406
287.631949	5224.975621	16.002471	-0.056785	3.921546
287.606542	5217.003284	16.007475	-0.056775	3.918683
287.522896	5208.978090	16.012480	-0.056754	3.915798
287.358882	5200.973381	16.017485	-0.056718	3.912917
287.386482	5192.938783	16.022490	-0.056718	3.910026
287.361156	5184.957917	16.027495	-0.056708	3.907151
287.455726	5176.981067	16.032499	-0.056721	3.904279
287.291917	5168.992323	16.037504	-0.056685	3.901394
287.379374	5160.967062	16.042509	-0.056696	3.898500
287.324807	5152.994911	16.047514	-0.056681	3.895619
287.196867	5144.967783	16.052519	-0.056652	3.892716
287.271608	5136.960178	16.057523	-0.056660	3.889821
287.182170	5128.973232	16.062528	-0.056638	3.886928
287.057041	5120.981251	16.067533	-0.056610	3.884030
287.036922	5113.002608	16.072538	-0.056601	3.881137
287.129125	5104.983492	16.077543	-0.056613	3.878230
286.919333	5097.003761	16.082547	-0.056569	3.875329
286.821996	5088.780971	16.087552	-0.056545	3.872339
286.942269	5080.781106	16.092557	-0.056562	3.869432
286.845134	5072.867616	16.097562	-0.056539	3.866551
286.709156	5064.876492	16.102567	-0.056509	3.863638
286.928771	5056.967075	16.107571	-0.056544	3.860760
286.925591	5048.968728	16.112576	-0.056539	3.857843
286.788496	5040.967566	16.117581	-0.056508	3.854919
286.861820	5033.013032	16.122586	-0.056516	3.852015
286.823370	5024.949437	16.127591	-0.056504	3.849067
286.713548	5016.985588	16.132595	-0.056478	3.846151
286.665004	5009.014182	16.137600	-0.056464	3.843232
286.641955	5001.003991	16.142605	-0.056454	3.840297
286.710001	4993.030569	16.147610	-0.056462	3.837374
286.383589	4985.016556	16.152615	-0.056396	3.834427
286.494121	4977.000271	16.157619	-0.056411	3.831485
286.484445	4968.994380	16.162624	-0.056404	3.828543
286.432597	4960.993664	16.167629	-0.056389	3.825599
286.476317	4953.061499	16.172634	-0.056392	3.822680
286.345219	4945.038661	16.177639	-0.056363	3.819722
286.304326	4937.059237	16.182643	-0.056350	3.816780
286.219099	4929.044564	16.187648	-0.056329	3.813821
286.285869	4921.016358	16.192653	-0.056336	3.810858
286.187618	4913.062243	16.197658	-0.056313	3.807917
286.184403	4905.021856	16.202663	-0.056307	3.804944
286.532172	4897.099613	16.207667	-0.056366	3.802019
286.296451	4889.080236	16.212672	-0.056317	3.799044
286.113601	4881.097814	16.217677	-0.056278	3.796081
286.294006	4873.073318	16.222682	-0.056306	3.793108
286.289181	4865.006341	16.227687	-0.056300	3.790113
286.134378	4857.042027	16.232691	-0.056266	3.787151
285.999207	4849.029971	16.237696	-0.056236	3.784169
285.900785	4841.072414	16.242701	-0.056212	3.781205
285.865993	4833.124025	16.247706	-0.056201	3.778245
285.623097	4825.066322	16.252711	-0.056150	3.775236
285.816407	4817.082484	16.257715	-0.056181	3.772262
285.835225	4809.019311	16.262720	-0.056179	3.769253
285.739602	4801.093166	16.267725	-0.056156	3.766289
285.767074	4793.079824	16.272730	-0.056156	3.763294
285.712123	4785.067896	16.277735	-0.056141	3.760294
285.699703	4777.104777	16.282739	-0.056133	3.757312
285.689189	4769.076267	16.287744	-0.056126	3.754303
285.651226	4761.083358	16.292749	-0.056114	3.751304
285.713260	4753.068217	16.297754	-0.056120	3.748296
285.659332	4745.063378	16.302759	-0.056105	3.745287
285.435858	4737.145299	16.307763	-0.056058	3.742305
285.359077	4729.082642	16.312768	-0.056039	3.739269
285.367449	4721.137236	16.317773	-0.056035	3.736277
285.297366	4713.129448	16.322778	-0.056017	3.733257
285.423305	4705.075257	16.327783	-0.056035	3.730222
285.355046	4697.137420	16.332787	-0.056017	3.727224
285.094564	4689.089373	16.337792	-0.055963	3.724176
285.078039	4681.138942	16.342797	-0.055955	3.721170
285.156748	4673.195459	16.347802	-0.055964	3.718165
284.952946	4665.180909	16.352807	-0.055921	3.715125
284.943806	4657.074052	16.357811	-0.055914	3.712052
285.118918	4649.042642	16.362816	-0.055942	3.709009
285.086079	4641.105182	16.367821	-0.055930	3.705994
284.904090	4633.160887	16.372826	-0.055891	3.702971
284.847849	4625.135386	16.377831	-0.055876	3.699917
285.004766	4617.205108	16.382835	-0.055900	3.696903
284.988410	4609.168882	16.387840	-0.055891	3.693841
284.738353	4601.158776	16.392845	-0.055840	3.690781
284.795482	4593.167907	16.397850	-0.055845	3.687733
284.801668	4585.136327	16.402855	-0.055841	3.684666
284.812307	4577.246679	16.407859	-0.055838	3.681651
284.849820	4569.201810	16.412864	-0.055840	3.678574
284.937334	4561.219832	16.417869	-0.055851	3.675521
284.945336	4553.215562	16.422874	-0.055847	3.672454
284.826147	4545.188261	16.427879	-0.055820	3.669372
284.689387	4537.248625	16.432883	-0.055789	3.666322
284.531804	4529.225266	16.437888	-0.055754	3.663236
284.623848	4521.199171	16.442893	-0.055766	3.660152
284.697575	4513.219165	16.447898	-0.055775	3.657084
284.532058	4505.232117	16.452903	-0.055739	3.654004
284.474392	4497.216999	16.457907	-0.055723	3.650913
284.431890	4489.210899	16.462912	-0.055710	3.647823
284.459375	4481.179325	16.467917	-0.055710	3.644723
284.345497	4473.288671	16.472922	-0.055683	3.641671
284.276473	4465.255543	16.477927	-0.055665	3.638562
284.365016	4457.278885	16.482931	-0.055676	3.635477
284.241232	4449.217360	16.487936	-0.055648	3.632351
284.378211	4441.189771	16.492941	-0.055668	3.629242
284.327627	4433.247225	16.497946	-0.055654	3.626158
284.111377	4425.233864	16.502951	-0.055608	3.623040
284.236271	4417.246126	16.507955	-0.055626	3.619938
284.048580	4409.276740	16.512960	-0.055586	3.616833
283.935851	4401.282557	16.517965	-0.055560	3.613717
283.828304	4393.297362	16.522970	-0.055535	3.610601
283.698977	4385.277456	16.527975	-0.055506	3.607469
283.982449	4377.289581	16.532979	-0.055553	3.604359
283.887470	4369.329073	16.537984	-0.055530	3.601245
283.838631	4361.337091	16.542989	-0.055516	3.598118
284.041351	4353.329268	16.547994	-0.055548	3.594990
283.901871	4345.328234	16.552999	-0.055517	3.591851
283.745600	4337.341839	16.558003	-0.055483	3.588715
283.660384	4329.308863	16.563008	-0.055462	3.585560
283.727960	4321.372031	16.568013	-0.055469	3.582444
283.845419	4313.367812	16.573018	-0.055486	3.579301
283.610477	4305.380384	16.578023	-0.055437	3.576151
283.597620	4297.392602	16.583027	-0.055429	3.573004
283.668532	4289.348736	16.588032	-0.055437	3.569836
283.661724	4281.384130	16.593037	-0.055431	3.566693
283.656365	4273.394836	16.598042	-0.055425	3.563538
283.423666	4265.395455	16.603047	-0.055376	3.560369
283.432816	4257.437472	16.608051	-0.055373	3.557221
283.650509	4249.373335	16.613056	-0.055408	3.554035
283.539616	4241.288809	16.618061	-0.055382	3.550828
283.541911	4233.343236	16.623066	-0.055377	3.547676
283.363929	4225.339608	16.628071	-0.055339	3.544493
283.355856	4217.429465	16.633075	-0.055332	3.541349
283.437329	4209.399581	16.638080	-0.055342	3.538158
283.239923	4201.391653	16.643085	-0.055300	3.534964
283.205519	4193.444530	16.648090	-0.055289	3.531797
283.154771	4185.399380	16.653095	-0.055274	3.528587
283.190906	4177.426122	16.658099	-0.055276	3.525405
283.160861	4169.446344	16.663104	-0.055265	3.522216
283.200705	4161.438825	16.668109	-0.055267	3.519015
283.147994	4153.475287	16.673114	-0.055252	3.515826
282.803408	4145.466616	16.678119	-0.055183	3.512607
283.028793	4137.450412	16.683123	-0.055219	3.509399
283.061360	4129.456305	16.688128	-0.055220	3.506192
282.863157	4121.488892	16.693133	-0.055178	3.502985
283.022580	4113.501163	16.698138	-0.055203	3.499778
282.789816	4105.520135	16.703143	-0.055154	3.496558
282.766179	4097.520991	16.708147	-0.055144	3.493335
282.873537	4089.505863	16.713152	-0.055159	3.490107
282.802955	4081.528269	16.718157	-0.055141	3.486885
282.844063	4073.564002	16.723162	-0.055143	3.483669
282.840997	4065.555754	16.728167	-0.055138	3.480431
282.829774	4057.580282	16.733171	-0.055130	3.477203
282.560007	4049.594911	16.738176	-0.055075	3.473959
282.334716	4041.559733	16.743181	-0.055028	3.470694
282.500392	4033.559613	16.748186	-0.055053	3.467452
282.444963	4025.549168	16.753191	-0.055038	3.464196
282.714029	4017.597902	16.758195	-0.055083	3.460972
282.376543	4009.604306	16.763200	-0.055015	3.457708
282.310906	4001.583600	16.768205	-0.054997	3.454438
282.242052	3993.599097	16.773210	-0.054979	3.451180
282.160280	3985.584985	16.778215	-0.054959	3.447906
282.268221	3977.583063	16.783219	-0.054974	3.444640
282.219298	3969.652511	16.788224	-0.054959	3.441396
282.228924	3961.640855	16.793229	-0.054956	3.438117
282.116976	3953.670343	16.798234	-0.054930	3.434847
281.950106	3945.620646	16.803239	-0.054894	3.431541
282.011597	3937.626261	16.808243	-0.054900	3.428261
281.929609	3929.629234	16.813248	-0.054879	3.424972
282.007563	3921.661697	16.818253	-0.054889	3.421698
282.178601	3913.671354	16.823258	-0.054915	3.418414
282.047952	3905.684729	16.828263	-0.054886	3.415118
281.899550	3897.710373	16.833267	-0.054853	3.411824
281.936269	3889.712577	16.838272	-0.054855	3.408523
281.956958	3881.676280	16.843277	-0.054853	3.405203
281.908352	3873.759946	16.848282	-0.054839	3.401926
281.967690	3865.736754	16.853287	-0.054845	3.398606
281.801131	3857.770392	16.858291	-0.054809	3.395298
281.665339	3849.696481	16.863296	-0.054778	3.391944
281.631907	3841.666352	16.868301	-0.054767	3.388607
281.627244	3833.717541	16.873306	-0.054761	3.385303
281.380067	3825.745234	16.878311	-0.054709	3.381977
281.444296	3817.769518	16.883315	-0.054716	3.378657
281.482967	3809.782828	16.888320	-0.054718	3.375328
281.096618	3801.804999	16.893325	-0.054641	3.371985
281.396068	3793.795502	16.898330	-0.054692	3.368649
281.354332	3785.795333	16.903335	-0.054679	3.365302
281.359778	3777.840108	16.908339	-0.054674	3.361972
281.334510	3769.820187	16.913344	-0.054665	3.358611
281.253472	3761.836169	16.918349	-0.054644	3.355259
281.259742	3753.825150	16.923354	-0.054640	3.351895
281.106412	3745.836700	16.928359	-0.054606	3.348532
281.377241	3737.823344	16.933363	-0.054652	3.345171
281.194185	3729.884712	16.938368	-0.054612	3.341821
281.236153	3721.891633	16.943373	-0.054615	3.338453
281.247298	3713.902636	16.948378	-0.054612	3.335082
281.169722	3705.879969	16.953383	-0.054592	3.331690
281.093799	3697.894149	16.958387	-0.054573	3.328311
280.810469	3689.914034	16.963392	-0.054515	3.324923
280.608575	3681.960808	16.968397	-0.054472	3.321545
280.862349	3673.955023	16.973402	-0.054514	3.318159
280.804259	3665.948820	16.978407	-0.054498	3.314758
280.763791	3657.945637	16.983411	-0.054485	3.311355
280.602098	3649.951187	16.988416	-0.054450	3.307947
280.744339	3641.924853	16.993421	-0.054471	3.304534
280.606155	3634.002723	16.998426	-0.054440	3.301152
280.501760	3626.007532	17.003431	-0.054416	3.297736
280.417641	3618.013023	17.008435	-0.054395	3.294317
280.415867	3610.017284	17.013440	-0.054389	3.290897
280.653711	3602.011977	17.018445	-0.054428	3.287479
280.479950	3594.037384	17.023450	-0.054391	3.284055
280.334824	3586.062793	17.028455	-0.054359	3.280629
280.298396	3578.102763	17.033459	-0.054347	3.277209
280.406587	3570.074085	17.038464	-0.054362	3.273761
280.315604	3562.064653	17.043469	-0.054340	3.270311
280.445959	3554.073274	17.048474	-0.054359	3.266873
280.473173	3546.059136	17.053479	-0.054358	3.263418
280.534286	3538.105309	17.058483	-0.054365	3.259987
280.320957	3530.155364	17.063488	-0.054320	3.256543
280.418509	3522.127703	17.068493	-0.054333	3.253073
280.275674	3514.142200	17.073498	-0.054301	3.249609
280.070613	3506.180376	17.078503	-0.054258	3.246149
280.019543	3498.212202	17.083507	-0.054243	3.242689
280.055599	3490.194228	17.088512	-0.054244	3.239206
279.903910	3482.215905	17.093517	-0.054211	3.235730
279.892580	3474.195924	17.098522	-0.054204	3.232237
279.971361	3466.126837	17.103527	-0.054213	3.228723
280.133602	3458.127356	17.108531	-0.054238	3.225239
279.750013	3450.221775	17.113536	-0.054161	3.221770
279.753670	3442.223680	17.118541	-0.054157	3.218272
279.898683	3434.228847	17.123546	-0.054179	3.214778
279.896727	3426.225143	17.128551	-0.054173	3.211270
279.685504	3418.272679	17.133555	-0.054129	3.207773
279.645964	3410.273702	17.138560	-0.054116	3.204257
279.672870	3402.294975	17.143565	-0.054116	3.200750
279.469402	3394.349675	17.148570	-0.054073	3.197244
279.416989	3386.315990	17.153575	-0.054058	3.193702
279.683262	3378.287060	17.158579	-0.054102	3.190171
279.673814	3370.320763	17.163584	-0.054095	3.186652
279.566837	3362.322495	17.168589	-0.054070	3.183111
279.600813	3354.374659	17.173594	-0.054071	3.179594
279.421171	3346.418797	17.178599	-0.054033	3.176061
279.354786	3338.394867	17.183603	-0.054015	3.172499
279.265354	3330.391342	17.188608	-0.053993	3.168940
279.429656	3322.394094	17.193613	-0.054018	3.165391
279.303450	3314.455590	17.198618	-0.053990	3.161852
279.088169	3306.472363	17.203623	-0.053945	3.158285
279.341663	3298.449207	17.208627	-0.053987	3.154717
279.142203	3290.444187	17.213632	-0.053944	3.151133
279.274203	3282.432083	17.218637	-0.053964	3.147556
279.256694	3274.470825	17.223642	-0.053955	3.143991
279.061240	3266.504014	17.228647	-0.053914	3.140412
279.011047	3258.524477	17.233651	-0.053899	3.136830
278.956700	3250.541990	17.238656	-0.053884	3.133242
278.882941	3242.499126	17.243661	-0.053865	3.129621
278.962032	3234.558628	17.248666	-0.053874	3.126050
278.754076	3226.578035	17.253671	-0.053830	3.122443
278.816283	3218.618710	17.258675	-0.053837	3.118854
278.733121	3210.620110	17.263680	-0.053816	3.115237
278.657082	3202.614960	17.268685	-0.053797	3.111612
278.861291	3194.608462	17.273690	-0.053829	3.107996
278.705212	3186.604505	17.278695	-0.053795	3.104360
278.543098	3178.677976	17.283699	-0.053760	3.100755
278.610064	3170.675984	17.288704	-0.053767	3.097121
278.501210	3162.674956	17.293709	-0.053742	3.093476
278.504684	3154.707042	17.298714	-0.053737	3.089847
278.540070	3146.693276	17.303719	-0.053738	3.086194
278.522403	3138.717577	17.308723	-0.053730	3.082551
278.337278	3130.763494	17.313728	-0.053690	3.078907
278.243097	3122.769477	17.318733	-0.053668	3.075243
278.467956	3114.694052	17.323738	-0.053704	3.071554
278.271424	3106.705812	17.328743	-0.053662	3.067880
278.260535	3098.724607	17.333747	-0.053655	3.064213
278.100772	3090.785141	17.338752	-0.053620	3.060554
278.044900	3082.796499	17.343757	-0.053605	3.056874
278.110739	3074.824651	17.348762	-0.053612	3.053202
277.861009	3066.825845	17.353767	-0.053560	3.049498
278.094153	3058.845900	17.358771	-0.053598	3.045822
277.990784	3050.894683	17.363776	-0.053574	3.042138
277.758237	3042.941582	17.368781	-0.053525	3.038443
278.009923	3034.925929	17.373786	-0.053567	3.034737
278.013111	3026.889953	17.378791	-0.053562	3.031006
277.906744	3018.926935	17.383795	-0.053537	3.027299
277.851551	3010.946280	17.388800	-0.053522	3.023581
277.874014	3002.964691	17.393805	-0.053521	3.019862
278.085484	2995.001918	17.398810	-0.053555	3.016156
277.815159	2986.989093	17.403815	-0.053499	3.012399
277.841489	2978.987962	17.408819	-0.053499	3.008658
277.665216	2971.027395	17.413824	-0.053461	3.004920
277.470730	2963.090716	17.418829	-0.053420	3.001189
277.542134	2955.116028	17.423834	-0.053428	2.997448
277.583363	2947.072160	17.428839	-0.053430	2.993668
277.612250	2939.066250	17.433843	-0.053430	2.989900
277.673587	2931.093453	17.438848	-0.053437	2.986146
277.610990	2923.110106	17.443853	-0.053420	2.982375
277.320888	2915.163751	17.448858	-0.053361	2.978605
277.356939	2907.154575	17.453863	-0.053362	2.974818
277.406378	2899.167983	17.458867	-0.053366	2.971037
277.432118	2891.185519	17.463872	-0.053366	2.967252
277.307231	2883.207045	17.468877	-0.053337	2.963456
277.262430	2875.251251	17.473882	-0.053324	2.959670
277.245485	2867.286282	17.478887	-0.053315	2.955877
277.236982	2859.267164	17.483891	-0.053309	2.952053
277.044920	2851.296565	17.488896	-0.053268	2.948238
277.009840	2843.295904	17.493901	-0.053256	2.944411
277.267878	2835.329298	17.498906	-0.053299	2.940611
277.049554	2827.377056	17.503911	-0.053253	2.936789
276.931605	2819.384707	17.508915	-0.053226	2.932947
276.963795	2811.356016	17.513920	-0.053227	2.929091
276.762784	2803.389924	17.518925	-0.053184	2.925247
276.719331	2795.468338	17.523930	-0.053171	2.921429
276.745601	2787.454428	17.528935	-0.053170	2.917564
276.749918	2779.439968	17.533939	-0.053166	2.913693
276.719532	2771.400629	17.538944	-0.053155	2.909802
276.520879	2763.434390	17.543949	-0.053113	2.905933
276.771847	2755.474295	17.548954	-0.053154	2.902086
276.747227	2747.486339	17.553959	-0.053145	2.898205
276.634760	2739.529727	17.558963	-0.053119	2.894330
276.598470	2731.560007	17.563968	-0.053107	2.890447
276.549524	2723.553795	17.568973	-0.053092	2.886541
276.282766	2715.636998	17.573978	-0.053037	2.882661
276.240761	2707.653625	17.578983	-0.053024	2.878755
276.351136	2699.659632	17.583987	-0.053040	2.874847
276.315670	2691.649491	17.588992	-0.053028	2.870918
276.215451	2683.688729	17.593997	-0.053004	2.867004
276.346958	2675.712882	17.599002	-0.053023	2.863091
276.177054	2667.721553	17.604007	-0.052987	2.859147
276.220703	2659.719820	17.609011	-0.052989	2.855205
276.131406	2651.759914	17.614016	-0.052968	2.851271
276.138789	2643.760356	17.619021	-0.052964	2.847317
276.147661	2635.807030	17.624026	-0.052960	2.843380
276.156234	2627.811881	17.629031	-0.052957	2.839417
276.005235	2619.898180	17.634035	-0.052923	2.835481
275.887099	2611.892021	17.639040	-0.052896	2.831494
275.659347	2603.886508	17.644045	-0.052849	2.827496
275.809932	2595.908698	17.649050	-0.052871	2.823528
275.806351	2587.920281	17.654055	-0.052866	2.819540
275.596378	2579.984911	17.659059	-0.052821	2.815561
275.569711	2571.983128	17.664064	-0.052811	2.811553
275.598066	2563.987065	17.669069	-0.052811	2.807546
275.558425	2556.039437	17.674074	-0.052799	2.803554
275.563663	2548.046472	17.679079	-0.052794	2.799535
275.778183	2540.065587	17.684083	-0.052829	2.795530
275.541908	2532.107351	17.689088	-0.052780	2.791503
275.349146	2524.112435	17.694093	-0.052739	2.787455
275.367817	2516.143558	17.699098	-0.052737	2.783426
275.309823	2508.155081	17.704103	-0.052721	2.779377
275.350384	2500.212315	17.709107	-0.052724	2.775351
275.391444	2492.194383	17.714112	-0.052726	2.771282
275.390458	2484.205386	17.719117	-0.052721	2.767218
275.228283	2476.266593	17.724122	-0.052685	2.763164
275.171747	2468.295350	17.729127	-0.052670	2.759094
275.256463	2460.327247	17.734131	-0.052680	2.755029
275.150108	2452.263465	17.739136	-0.052655	2.750896
274.734533	2444.334748	17.744141	-0.052573	2.746808
275.237712	2436.329681	17.749146	-0.052661	2.742731
274.962038	2428.377937	17.754151	-0.052604	2.738627
274.781807	2420.433022	17.759155	-0.052566	2.734527
274.765266	2412.427454	17.764160	-0.052557	2.730399
274.939812	2404.422778	17.769165	-0.052585	2.726277
274.897583	2396.488484	17.774170	-0.052572	2.722172
274.673956	2388.546837	17.779175	-0.052525	2.718045
274.853677	2380.552980	17.784179	-0.052553	2.713911
274.740302	2372.556401	17.789184	-0.052527	2.709750
274.448126	2364.603775	17.794189	-0.052467	2.705595
274.415435	2356.653957	17.799194	-0.052456	2.701450
274.498820	2348.639039	17.804199	-0.052466	2.697273
274.634739	2340.660009	17.809203	-0.052486	2.693112
274.424556	2332.702174	17.814208	-0.052442	2.688933
274.263961	2324.723469	17.819213	-0.052407	2.684740
274.218057	2316.798701	17.824218	-0.052393	2.680575
274.244425	2308.824131	17.829223	-0.052393	2.676383
274.383511	2300.793286	17.834227	-0.052414	2.672162
274.271210	2292.819193	17.839232	-0.052388	2.667948
274.043433	2284.850561	17.844237	-0.052340	2.663723
274.165489	2276.895088	17.849242	-0.052358	2.659520
274.391871	2268.893478	17.854247	-0.052394	2.655293
274.183429	2260.932377	17.859251	-0.052350	2.651053
274.057913	2252.961071	17.864256	-0.052322	2.646806
274.034785	2244.996220	17.869261	-0.052312	2.642562
274.093597	2237.041124	17.874266	-0.052318	2.638322
274.117839	2229.067422	17.879271	-0.052318	2.634062
273.916577	2221.083392	17.884275	-0.052275	2.629776
274.027330	2213.116168	17.889280	-0.052290	2.625512
273.795028	2205.153106	17.894285	-0.052242	2.621221
273.900483	2197.187496	17.899290	-0.052256	2.616943
274.051930	2189.188319	17.904295	-0.052279	2.612644
273.924154	2181.226491	17.909299	-0.052250	2.608339
273.666269	2173.282232	17.914304	-0.052197	2.604028
273.628045	2165.303745	17.919309	-0.052185	2.599706
273.668759	2157.369823	17.924314	-0.052187	2.595406
273.362702	2149.243715	17.929319	-0.052125	2.590971
273.417094	2141.241647	17.934323	-0.052130	2.586620
273.462582	2133.298473	17.939328	-0.052133	2.582293
273.380682	2125.366005	17.944333	-0.052113	2.577957
273.360219	2117.425516	17.949338	-0.052104	2.573613
273.476593	2109.424268	17.954343	-0.052120	2.569237
273.445130	2101.482791	17.959347	-0.052109	2.564877
273.309075	2093.566058	17.964352	-0.052079	2.560516
273.238610	2085.607574	17.969357	-0.052060	2.556129
273.368891	2077.615017	17.974362	-0.052079	2.551729
273.130882	2069.650717	17.979367	-0.052030	2.547312
273.208103	2061.682851	17.984371	-0.052039	2.542907
273.285377	2053.707635	17.989376	-0.052048	2.538490
273.166707	2045.764205	17.994381	-0.052021	2.534070
272.995518	2037.795717	17.999386	-0.051984	2.529624
273.020730	2029.822101	18.004391	-0.051983	2.525182
272.913084	2021.880067	18.009395	-0.051958	2.520739
272.964107	2013.927284	18.014400	-0.051963	2.516294
272.979171	2005.896276	18.019405	-0.051960	2.511795
272.908933	1997.940346	18.024410	-0.051942	2.507324
272.789985	1989.978850	18.029415	-0.051915	2.502838
272.802955	1982.022426	18.034419	-0.051912	2.498357
272.700112	1974.085557	18.039424	-0.051888	2.493870
272.598447	1966.096399	18.044429	-0.051863	2.489345
272.643439	1958.145219	18.049434	-0.051867	2.484845
272.651361	1950.178592	18.054439	-0.051863	2.480325
272.531759	1942.246891	18.059443	-0.051835	2.475807
272.366770	1934.266093	18.064448	-0.051800	2.471249
272.246157	1926.293782	18.069453	-0.051772	2.466691
272.432566	1918.320745	18.074458	-0.051801	2.462147
272.175801	1910.385663	18.079463	-0.051748	2.457583
272.190968	1902.415191	18.084467	-0.051746	2.453011
272.226110	1894.441207	18.089472	-0.051747	2.448430
272.111739	1886.481986	18.094477	-0.051721	2.443837
271.942176	1878.572888	18.099482	-0.051684	2.439261
272.090638	1870.573181	18.104487	-0.051707	2.434647
272.146039	1862.514650	18.109491	-0.051712	2.429984
272.040496	1854.585786	18.114496	-0.051687	2.425375
271.794309	1846.652304	18.119501	-0.051636	2.420743
271.779211	1838.720940	18.124506	-0.051628	2.416122
271.789694	1830.726545	18.129511	-0.051625	2.411456
271.939284	1822.741122	18.134515	-0.051647	2.406798
271.920077	1814.808685	18.139520	-0.051639	2.402149
271.861728	1806.861495	18.144525	-0.051623	2.397479
271.482691	1798.950341	18.149530	-0.051547	2.392796
271.542220	1790.947352	18.154535	-0.051553	2.388084
271.476801	1782.991885	18.159539	-0.051535	2.383380
271.593015	1775.043888	18.164544	-0.051552	2.378687
271.605653	1767.069895	18.169549	-0.051549	2.373960
271.827923	1759.082802	18.174554	-0.051585	2.369233
271.640100	1751.136301	18.179559	-0.051545	2.364488
271.463654	1743.225249	18.184563	-0.051507	2.359756
271.470914	1735.290763	18.189568	-0.051503	2.355014
271.421751	1727.286645	18.194573	-0.051489	2.350217
271.452718	1719.322867	18.199578	-0.051489	2.345441
271.200960	1711.386894	18.204583	-0.051437	2.340648
271.172507	1703.446334	18.209587	-0.051427	2.335861
271.128591	1695.492393	18.214592	-0.051413	2.331055
271.212395	1687.500373	18.219597	-0.051424	2.326227
271.206540	1679.570281	18.224602	-0.051418	2.321418
270.998632	1671.643643	18.229607	-0.051374	2.316585
271.096236	1663.660659	18.234611	-0.051387	2.311733
271.028766	1655.699832	18.239616	-0.051369	2.306871
270.933970	1647.754215	18.244621	-0.051346	2.302005
270.830917	1639.832437	18.249626	-0.051322	2.297143
270.821513	1631.861025	18.254631	-0.051315	2.292248
270.810684	1623.899990	18.259635	-0.051308	2.287348
270.728394	1615.981789	18.264640	-0.051287	2.282459
270.800362	1608.010350	18.269645	-0.051295	2.277539
270.709365	1600.042345	18.274650	-0.051273	2.272597
270.507638	1592.056050	18.279655	-0.051231	2.267623
270.358050	1584.128809	18.284659	-0.051197	2.262679
270.508767	1576.173290	18.289664	-0.051220	2.257733
270.420189	1568.217687	18.294669	-0.051199	2.252755
270.358091	1560.271298	18.299674	-0.051182	2.247774
270.335595	1552.327837	18.304679	-0.051173	2.242787
270.390986	1544.391915	18.309683	-0.051178	2.237801
270.135357	1536.461693	18.314688	-0.051125	2.232780
270.185146	1528.479818	18.319693	-0.051129	2.227742
270.270123	1520.534166	18.324698	-0.051140	2.222719
270.250276	1512.597283	18.329703	-0.051131	2.217680
270.114710	1504.660628	18.334707	-0.051100	2.212620
270.224565	1496.703020	18.339712	-0.051116	2.207556
270.242454	1488.748476	18.344717	-0.051114	2.202475
269.910598	1480.875009	18.349722	-0.051047	2.197403
270.057391	1472.873119	18.354727	-0.051069	2.192279
269.840535	1464.935461	18.359731	-0.051024	2.187152
270.021158	1456.976183	18.364736	-0.051052	2.182035
269.700820	1449.075646	18.369741	-0.050987	2.176898
269.961780	1441.089959	18.374746	-0.051031	2.171747
269.874821	1433.143472	18.379751	-0.051009	2.166577
269.727836	1425.228381	18.384755	-0.050977	2.161410
269.679849	1417.322243	18.389760	-0.050963	2.156246
269.742580	1409.332741	18.394765	-0.050969	2.151024
269.593228	1401.412882	18.399770	-0.050936	2.145816
269.297159	1393.509643	18.404775	-0.050876	2.140592
269.321954	1385.557633	18.409779	-0.050875	2.135354
269.374823	1377.593930	18.414784	-0.050880	2.130098
269.311313	1369.647024	18.419789	-0.050863	2.124828
269.382756	1361.735647	18.424794	-0.050871	2.119582
269.273949	1353.810984	18.429799	-0.050846	2.114297
269.363055	1345.763601	18.434803	-0.050857	2.108936
269.287998	1337.867066	18.439808	-0.050838	2.103646
269.013651	1329.955355	18.444813	-0.050782	2.098314
269.021440	1322.026981	18.449818	-0.050778	2.092984
268.876179	1314.090808	18.454823	-0.050746	2.087620
268.907605	1306.168123	18.459827	-0.050746	2.082268
268.900190	1298.257147	18.464832	-0.050740	2.076908
268.841235	1290.296066	18.469837	-0.050724	2.071493
268.942391	1282.346418	18.474842	-0.050737	2.066089
268.956503	1274.415351	18.479847	-0.050735	2.060674
268.785513	1266.517378	18.484851	-0.050698	2.055250
268.564342	1258.607525	18.489856	-0.050652	2.049797
268.589603	1250.657351	18.494861	-0.050651	2.044327
268.609800	1242.746546	18.499866	-0.050650	2.038869
268.587547	1234.808614	18.504871	-0.050640	2.033374
268.530728	1226.851174	18.509875	-0.050625	2.027846
268.405239	1218.939690	18.514880	-0.050596	2.022328
268.419487	1211.007121	18.519885	-0.050594	2.016795
268.483977	1203.076380	18.524890	-0.050600	2.011253
268.470765	1195.137596	18.529895	-0.050593	2.005682
268.424370	1187.225773	18.534899	-0.050579	2.000111
268.543844	1179.312050	18.539904	-0.050596	1.994540
268.274445	1171.386224	18.544909	-0.050541	1.988904
268.322997	1163.465620	18.549914	-0.050545	1.983290
268.229116	1155.558147	18.554919	-0.050522	1.977654
268.068928	1147.650388	18.559923	-0.050487	1.971994
268.243118	1139.695008	18.564928	-0.050514	1.966320
268.081978	1131.796937	18.569933	-0.050479	1.960635
268.015062	1123.917296	18.574938	-0.050462	1.954956
267.846567	1115.957692	18.579943	-0.050425	1.949192
267.957502	1107.998518	18.584947	-0.050440	1.943442
267.922951	1100.108475	18.589952	-0.050429	1.937708
267.683804	1092.199813	18.594957	-0.050379	1.931922
267.690009	1084.282300	18.599962	-0.050375	1.926139
267.438723	1076.406114	18.604967	-0.050323	1.920341
267.461988	1068.487173	18.609971	-0.050322	1.914523
267.649918	1060.521032	18.614976	-0.050352	1.908672
267.381269	1052.635643	18.619981	-0.050297	1.902811
267.384554	1044.744005	18.624986	-0.050293	1.896958
267.444035	1036.799650	18.629991	-0.050299	1.891054
267.274351	1028.902963	18.634995	-0.050262	1.885141
267.286972	1021.023390	18.640000	-0.050259	1.879243
267.229232	1013.104529	18.645005	-0.050243	1.873289
267.251103	1005.157338	18.650010	-0.050242	1.867304
267.162376	997.266698	18.655015	-0.050220	1.861329
267.072406	989.379428	18.660019	-0.050198	1.855338
267.055093	981.474382	18.665024	-0.050190	1.849322
266.986870	973.564051	18.670029	-0.050172	1.843276
266.905326	965.694559	18.675034	-0.050152	1.837241
266.995144	957.758077	18.680039	-0.050163	1.831154
266.917877	949.841647	18.685043	-0.050144	1.825042
266.830789	941.991761	18.690048	-0.050123	1.818960
266.809888	934.079232	18.695053	-0.050114	1.812817
266.793706	926.172959	18.700058	-0.050105	1.806659
266.684450	918.302033	18.705063	-0.050080	1.800496
266.558459	910.421750	18.710067	-0.050051	1.794302
266.688067	902.449282	18.715072	-0.050070	1.788045
266.436207	894.587282	18.720077	-0.050018	1.781807
266.454688	886.703099	18.725082	-0.050017	1.775563
266.311116	878.823212	18.730087	-0.049985	1.769280
266.252098	870.940063	18.735091	-0.049969	1.762982
266.299327	863.068313	18.740096	-0.049972	1.756684
266.290372	855.148169	18.745101	-0.049965	1.750318
266.319642	847.257580	18.750106	-0.049966	1.743957
266.211986	839.400789	18.755111	-0.049941	1.737583
266.142366	831.515333	18.760115	-0.049922	1.731167
266.190228	823.634948	18.765120	-0.049926	1.724746
265.961456	815.785996	18.770125	-0.049879	1.718291
265.839706	807.913834	18.775130	-0.049851	1.711807
265.959025	799.999576	18.780135	-0.049868	1.705294
265.816131	792.143013	18.785139	-0.049836	1.698770
265.726060	784.277069	18.790144	-0.049814	1.692220
265.548343	776.399834	18.795149	-0.049776	1.685624
265.761402	768.522175	18.800154	-0.049811	1.679053
265.539175	760.681848	18.805159	-0.049764	1.672430
265.429213	752.795328	18.810163	-0.049738	1.665756
265.585854	744.921435	18.815168	-0.049762	1.659102
265.394960	737.073621	18.820173	-0.049722	1.652396
265.255850	729.221475	18.825178	-0.049691	1.645667
264.975744	721.413304	18.830183	-0.049634	1.638928
265.042229	713.496621	18.835187	-0.049641	1.632115
264.978755	705.606628	18.840192	-0.049624	1.625279
264.843789	697.768084	18.845197	-0.049594	1.618449
264.916896	689.897943	18.850202	-0.049602	1.611591
264.933772	682.030360	18.855207	-0.049600	1.604699
264.837294	674.206027	18.860211	-0.049577	1.597799
264.869986	666.348410	18.865216	-0.049578	1.590857
264.921268	658.471285	18.870221	-0.049582	1.583871
264.748355	650.673481	18.875226	-0.049545	1.576892
264.853133	642.804116	18.880231	-0.049560	1.569858
264.708666	634.985518	18.885235	-0.049528	1.562802
264.691272	627.171071	18.890240	-0.049519	1.555736
264.367068	619.342271	18.895245	-0.049454	1.548580
264.425413	611.498156	18.900250	-0.049460	1.541433
264.435144	603.658398	18.905255	-0.049456	1.534250
264.330866	595.824571	18.910259	-0.049432	1.527021
264.347064	588.008774	18.915264	-0.049430	1.519793
264.410559	580.167735	18.920269	-0.049436	1.512513
264.397067	572.331489	18.925274	-0.049429	1.505192
264.202944	564.552999	18.930279	-0.049388	1.497861
264.014815	556.738778	18.935283	-0.049347	1.490461
264.372051	548.881303	18.940288	-0.049409	1.483068
264.057966	541.125570	18.945293	-0.049345	1.475630
263.994684	533.270516	18.950298	-0.049328	1.468098
263.848830	525.481275	18.955303	-0.049296	1.460578
263.832914	517.678836	18.960307	-0.049288	1.453027
263.783652	509.875132	18.965312	-0.049274	1.445429
263.718543	502.093044	18.970317	-0.049257	1.437811
263.654803	494.293975	18.975322	-0.049240	1.430135
263.476219	486.522156	18.980327	-0.049201	1.422426
263.451417	478.735973	18.985331	-0.049192	1.414685
263.523155	470.927720	18.990336	-0.049200	1.406896
263.152613	463.209139	18.995341	-0.049126	1.399081
263.434215	455.366372	19.000346	-0.049173	1.391205
263.183782	447.613149	19.005351	-0.049122	1.383285
262.910795	439.881928	19.010355	-0.049066	1.375338
263.005162	432.082826	19.015360	-0.049078	1.367339
262.869945	424.330936	19.020365	-0.049048	1.359301
262.878255	416.567921	19.025370	-0.049045	1.351229
262.835347	408.805254	19.030375	-0.049031	1.343100
262.758638	401.058707	19.035379	-0.049012	1.334932
262.823485	393.295644	19.040384	-0.049019	1.326722
262.632459	385.583195	19.045389	-0.048979	1.318468
262.563011	377.760768	19.050394	-0.048961	1.310067
262.549459	369.978780	19.055399	-0.048953	1.301665
262.375314	362.286072	19.060403	-0.048916	1.293276
262.390869	354.556503	19.065408	-0.048913	1.284827
262.347543	346.853158	19.070413	-0.048900	1.276340
262.316663	339.134605	19.075418	-0.048890	1.267782
262.216045	331.445163	19.080423	-0.048866	1.259184
262.051007	323.755322	19.085427	-0.048830	1.250515
262.248786	316.036615	19.090432	-0.048862	1.241823
261.875349	308.396562	19.095437	-0.048787	1.233048
262.050076	300.654493	19.100442	-0.048815	1.224200
262.028006	292.978522	19.105447	-0.048806	1.215325
261.754479	285.334195	19.110451	-0.048750	1.206373
261.598805	277.700991	19.115456	-0.048716	1.197390
261.566453	270.020853	19.120461	-0.048705	1.188308
261.610555	262.361267	19.125466	-0.048708	1.179196
261.527276	254.718058	19.130471	-0.048688	1.170007
261.435303	247.081327	19.135475	-0.048665	1.160751
261.504766	239.421492	19.140480	-0.048673	1.151426
261.271281	231.796119	19.145485	-0.048625	1.142004
261.191219	224.184563	19.150490	-0.048605	1.132553
261.250115	216.557210	19.155495	-0.048611	1.123032
261.067346	208.978160	19.160499	-0.048572	1.113439
261.041102	201.379299	19.165504	-0.048562	1.103771
260.854920	193.817366	19.170509	-0.048523	1.094030
260.903703	186.220117	19.175514	-0.048527	1.084208
260.853255	178.665177	19.180519	-0.048513	1.074330
260.889267	171.079041	19.185523	-0.048514	1.064338
260.767062	163.554143	19.190528	-0.048487	1.054296
260.704368	156.010098	19.195533	-0.048470	1.044147
260.629873	148.507037	19.200538	-0.048451	1.033950
260.487909	140.998841	19.205543	-0.048420	1.023629
260.444060	133.497228	19.210547	-0.048407	1.013235
260.410085	126.011703	19.215552	-0.048396	1.002759
260.216241	118.550247	19.220557	-0.048355	0.992167
260.147321	111.063658	19.225562	-0.048337	0.981455
259.999620	103.629886	19.230567	-0.048305	0.970682
259.990057	96.183175	19.235571	-0.048298	0.959804
260.024713	88.752216	19.240576	-0.048300	0.948837
259.793024	81.377320	19.245581	-0.048252	0.937755
259.791531	73.975077	19.250586	-0.048247	0.926561
259.727271	66.616491	19.255591	-0.048230	0.915279
259.480034	59.507273	19.260595	-0.048179	0.904196