Fri Mar 12 12:21:35 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.497623	0.003685	0.000000	0.000011	0.721118
0.645541	-0.061949	0.005005	-0.000017	0.721041
0.533219	-0.130502	0.010010	0.000004	0.720867
0.598654	-0.138044	0.015014	-0.000008	0.720875
0.430270	-0.108112	0.020019	0.000024	0.720875
0.470684	-0.117663	0.025024	0.000016	0.720870
0.607723	-0.137480	0.030029	-0.000009	0.720879
0.438735	-0.113708	0.035034	0.000022	0.720867
0.304801	-0.089277	0.040038	0.000047	0.720868
0.255638	-0.078830	0.045043	0.000056	0.720871
0.398712	-0.106981	0.050048	0.000029	0.720866
0.595818	-0.138128	0.055053	-0.000007	0.720874
0.514613	-0.125308	0.060058	0.000008	0.720871
0.577509	-0.136126	0.065062	-0.000004	0.720871
0.602701	-0.138960	0.070067	-0.000009	0.720875
0.632570	-0.148379	0.075072	-0.000014	0.720867
0.538719	-0.247521	0.080077	0.000003	0.720639
0.541190	-0.302650	0.085082	0.000003	0.720531
0.578635	-0.307866	0.090086	-0.000004	0.720534
0.459408	-0.285339	0.095091	0.000018	0.720537
0.588912	-0.311707	0.100096	-0.000006	0.720530
0.558769	-0.301199	0.105101	-0.000000	0.720540
0.377585	-0.320484	0.110106	0.000033	0.720439
0.481222	-0.449771	0.115110	0.000014	0.720221
0.539885	-0.457974	0.120115	0.000003	0.720225
0.570411	-0.466515	0.125120	-0.000003	0.720219
0.583101	-0.465064	0.130125	-0.000005	0.720226
0.544392	-0.524874	0.135130	0.000002	0.720095
0.596667	-0.635615	0.140134	-0.000007	0.719895
0.487682	-0.613526	0.145139	0.000013	0.719900
0.577364	-0.633077	0.150144	-0.000004	0.719893
0.694857	-0.689703	0.155149	-0.000026	0.719823
0.297965	-0.732924	0.160154	0.000048	0.719599
0.346007	-0.741019	0.165158	0.000039	0.719600
0.399421	-0.750348	0.170163	0.000029	0.719600
0.517462	-0.851119	0.175168	0.000007	0.719443
0.581881	-0.949882	0.180173	-0.000005	0.719271
0.486980	-0.936121	0.185178	0.000013	0.719264
0.438973	-0.946225	0.190182	0.000022	0.719228
0.431253	-1.079864	0.195187	0.000023	0.718961
0.322859	-1.062987	0.200192	0.000044	0.718957
0.461178	-1.083522	0.205197	0.000018	0.718965
0.209489	-1.204029	0.210202	0.000065	0.718638
0.012228	-1.167565	0.215206	0.000102	0.718641
0.309175	-1.219083	0.220211	0.000046	0.718644
0.287670	-1.362727	0.225216	0.000050	0.718353
0.286737	-1.361271	0.230221	0.000050	0.718355
0.386262	-1.416361	0.235226	0.000032	0.718282
0.407738	-1.556800	0.240230	0.000028	0.718012
0.380114	-1.545850	0.245235	0.000033	0.718024
0.185819	-1.617714	0.250240	0.000069	0.717813
0.238511	-1.680982	0.255245	0.000060	0.717707
0.255798	-1.708163	0.260250	0.000056	0.717659
0.116551	-1.826645	0.265254	0.000082	0.717376
0.156274	-1.831643	0.270259	0.000075	0.717380
0.182496	-1.947266	0.275264	0.000070	0.717161
0.043537	-1.961789	0.280269	0.000096	0.717083
-0.121683	-1.994746	0.285274	0.000127	0.716960
-0.210975	-2.084483	0.290278	0.000143	0.716751
-0.370600	-2.057995	0.295283	0.000173	0.716747
-0.404014	-2.208823	0.300288	0.000179	0.716437
-0.174439	-2.244449	0.305293	0.000137	0.716447
-0.470788	-2.315786	0.310298	0.000192	0.716201
-0.535061	-2.341824	0.315302	0.000204	0.716127
-2.019751	-2.136026	0.320307	0.000480	0.716011
-2.864661	-2.054738	0.325312	0.000637	0.715874
-2.528959	-2.110339	0.330317	0.000575	0.715882
-2.704019	-2.156555	0.335322	0.000608	0.715729
-4.248805	-1.976108	0.340326	0.000895	0.715541
-3.684515	-2.076804	0.345331	0.000790	0.715541
-3.710497	-2.074355	0.350336	0.000795	0.715536
-4.520159	-2.075797	0.355341	0.000946	0.715247
-4.877026	-2.025773	0.360346	0.001012	0.715221
-4.900769	-2.019472	0.365350	0.001016	0.715225
-4.676144	-2.056433	0.370355	0.000975	0.715231
-5.604679	-2.052755	0.375360	0.001147	0.714910
-5.815565	-2.015868	0.380365	0.001187	0.714909
-5.900235	-2.004967	0.385370	0.001202	0.714900
-5.837450	-2.015734	0.390374	0.001191	0.714901
-5.597302	-2.112802	0.395379	0.001146	0.714793
-7.073676	-1.949466	0.400384	0.001421	0.714596
-6.395514	-2.065620	0.405389	0.001295	0.714605
-6.644071	-2.025559	0.410394	0.001341	0.714597
-6.775400	-2.001468	0.415398	0.001365	0.714598
-6.504011	-2.124675	0.420403	0.001315	0.714449
-8.140907	-1.925375	0.425408	0.001619	0.714266
-7.283623	-2.073210	0.430413	0.001460	0.714276
-7.384900	-2.059307	0.435418	0.001479	0.714268
-8.160848	-1.919507	0.440422	0.001623	0.714271
-7.295407	-2.072961	0.445427	0.001462	0.714272
-8.198061	-2.069532	0.450432	0.001630	0.713959
-8.558165	-2.002208	0.455437	0.001697	0.713966
-8.896718	-1.945871	0.460442	0.001760	0.713958
-8.262981	-2.058323	0.465446	0.001642	0.713959
-8.477270	-2.017606	0.470451	0.001682	0.713964
-8.832413	-1.958471	0.475456	0.001748	0.713956
-9.007838	-2.082293	0.480461	0.001781	0.713647
-9.216090	-2.047520	0.485466	0.001820	0.713643
-9.956326	-1.915295	0.490470	0.001957	0.713644
-9.274837	-2.035079	0.495475	0.001830	0.713647
-9.457732	-2.005020	0.500480	0.001865	0.713642
-9.723567	-1.953706	0.505485	0.001914	0.713650
-9.815132	-2.032121	0.510490	0.001931	0.713461
-10.644353	-1.939530	0.515494	0.002085	0.713352
-10.276945	-2.001592	0.520499	0.002017	0.713359
-10.724383	-1.926242	0.525504	0.002100	0.713350
-10.458161	-1.969725	0.530509	0.002051	0.713358
-10.151006	-2.026035	0.535514	0.001994	0.713355
-10.633623	-1.938217	0.540518	0.002083	0.713358
-10.947057	-2.031075	0.545523	0.002142	0.713063
-11.377993	-1.979018	0.550528	0.002222	0.713013
-11.353640	-1.977998	0.555533	0.002217	0.713024
-11.638006	-1.930954	0.560538	0.002270	0.713017
-11.379774	-1.974586	0.565542	0.002222	0.713022
-11.107997	-2.021612	0.570547	0.002172	0.713024
-11.594998	-1.939326	0.575552	0.002262	0.713016
-11.644308	-2.066702	0.580557	0.002271	0.712745
-12.011341	-2.021039	0.585562	0.002340	0.712705
-12.365446	-1.959096	0.590566	0.002406	0.712703
-12.203688	-1.983580	0.595571	0.002376	0.712712
-12.291591	-1.973224	0.600576	0.002392	0.712701
-12.313962	-1.966116	0.605581	0.002396	0.712707
-12.243979	-1.988165	0.610586	0.002383	0.712688
-12.924955	-2.020402	0.615590	0.002510	0.712383
-13.032758	-1.998308	0.620595	0.002530	0.712388
-13.678609	-1.888140	0.625600	0.002650	0.712379
-13.199668	-1.968008	0.630605	0.002561	0.712389
-12.952843	-2.015333	0.635610	0.002515	0.712383
-13.580511	-1.904840	0.640614	0.002632	0.712380
-13.223460	-1.965183	0.645619	0.002565	0.712387
-13.398813	-2.040870	0.650624	0.002598	0.712174
-13.992013	-1.975608	0.655629	0.002708	0.712093
-14.121869	-1.955068	0.660634	0.002732	0.712088
-13.869836	-1.999991	0.665638	0.002686	0.712088
-13.481343	-2.067036	0.670643	0.002613	0.712092
-13.862488	-2.005050	0.675648	0.002684	0.712081
-13.759026	-2.058318	0.680653	0.002665	0.712011
-14.828445	-1.996948	0.685658	0.002864	0.711754
-14.854618	-1.990458	0.690662	0.002869	0.711757
-15.198080	-1.925787	0.695667	0.002933	0.711764
-15.225218	-1.926289	0.700672	0.002938	0.711754
-14.776413	-2.002910	0.705677	0.002854	0.711760
-15.220983	-1.926172	0.710682	0.002937	0.711756
-15.049786	-1.956848	0.715686	0.002905	0.711755
-14.830855	-2.114590	0.720691	0.002864	0.711519
-16.303035	-1.887608	0.725696	0.003138	0.711448
-16.098043	-1.919572	0.730701	0.003100	0.711457
-15.380238	-2.050195	0.735706	0.002967	0.711452
-15.879431	-1.962313	0.740710	0.003059	0.711450
-15.971500	-1.942673	0.745715	0.003077	0.711456
-15.706188	-1.994934	0.750720	0.003027	0.711446
-15.788654	-2.097351	0.755725	0.003043	0.711213
-17.005187	-1.918757	0.760730	0.003269	0.711136
-17.131137	-1.898088	0.765734	0.003292	0.711133
-16.302310	-2.042629	0.770739	0.003138	0.711139
-16.803714	-1.957792	0.775744	0.003231	0.711130
-17.122187	-1.895423	0.780749	0.003291	0.711142
-16.807669	-1.955004	0.785754	0.003232	0.711135
-16.989773	-1.981543	0.790758	0.003266	0.711017
-17.779895	-1.913603	0.795763	0.003413	0.710871
-17.289960	-2.003074	0.800768	0.003322	0.710867
-17.327457	-1.992028	0.805773	0.003329	0.710876
-17.720579	-1.923121	0.810778	0.003402	0.710874
-17.894759	-1.894285	0.815782	0.003434	0.710869
-17.492940	-1.963754	0.820787	0.003360	0.710874
-17.733754	-1.997867	0.825792	0.003405	0.710720
-18.761092	-1.908565	0.830797	0.003596	0.710533
-18.060461	-2.035116	0.835802	0.003465	0.710529
-18.338371	-1.985449	0.840806	0.003517	0.710529
-18.330470	-1.982612	0.845811	0.003516	0.710538
-18.580248	-1.943663	0.850816	0.003562	0.710527
-18.327290	-1.983480	0.855821	0.003515	0.710537
-18.548597	-2.034197	0.860826	0.003556	0.710357
-19.871574	-1.869970	0.865830	0.003802	0.710214
-18.980301	-2.024365	0.870835	0.003637	0.710223
-19.375104	-1.958162	0.875840	0.003710	0.710215
-19.749593	-1.887181	0.880845	0.003780	0.710224
-19.517976	-1.930971	0.885850	0.003737	0.710219
-19.306388	-1.969747	0.890854	0.003697	0.710216
-19.356376	-2.016313	0.895859	0.003706	0.710106
-20.464537	-1.926764	0.900864	0.003913	0.709890
-19.983940	-2.008094	0.905869	0.003823	0.709899
-20.374245	-1.941244	0.910874	0.003896	0.709893
-20.606725	-1.900725	0.915878	0.003939	0.709891
-19.990264	-2.008141	0.920883	0.003824	0.709896
-20.439605	-1.932567	0.925888	0.003908	0.709887
-20.569129	-1.919921	0.930893	0.003932	0.709867
-21.010944	-1.977338	0.935898	0.004014	0.709594
-21.091090	-1.964161	0.940902	0.004029	0.709592
-21.504842	-1.888057	0.945907	0.004106	0.709597
-21.453234	-1.900001	0.950912	0.004097	0.709591
-21.126736	-1.955744	0.955917	0.004036	0.709596
-21.181144	-1.946803	0.960922	0.004046	0.709595
-21.421171	-1.904509	0.965926	0.004091	0.709594
-21.046723	-2.075863	0.970931	0.004021	0.709385
-22.278241	-1.917052	0.975936	0.004250	0.709263
-22.033816	-1.957898	0.980941	0.004205	0.709269
-22.210767	-1.928053	0.985946	0.004238	0.709265
-22.500234	-1.879481	0.990950	0.004291	0.709259
-22.113525	-1.942954	0.995955	0.004220	0.709270
-22.358620	-1.903110	1.000960	0.004265	0.709263
-22.069362	-2.022030	1.005965	0.004211	0.709128
-22.879289	-1.964647	1.010970	0.004362	0.708954
-23.141006	-1.917588	1.015974	0.004411	0.708955
-23.024517	-1.936297	1.020979	0.004389	0.708959
-22.943557	-1.953508	1.025984	0.004374	0.708953
-23.250060	-1.897025	1.030989	0.004431	0.708957
-22.898227	-1.959861	1.035994	0.004366	0.708957
-22.826948	-2.045438	1.040998	0.004352	0.708811
-23.768337	-1.961425	1.046003	0.004528	0.708643
-24.179225	-1.891441	1.051008	0.004604	0.708637
-24.001602	-1.920268	1.056013	0.004571	0.708642
-23.474766	-2.016518	1.061018	0.004473	0.708638
-24.032832	-1.917809	1.066022	0.004577	0.708636
-23.665692	-1.978894	1.071027	0.004508	0.708645
-23.788552	-2.029134	1.076032	0.004531	0.708500
-25.051470	-1.877566	1.081037	0.004766	0.708353
-24.781375	-1.928252	1.086042	0.004716	0.708348
-24.826411	-1.921953	1.091046	0.004724	0.708345
-24.480712	-1.978947	1.096051	0.004660	0.708354
-24.780244	-1.929782	1.101056	0.004716	0.708346
-24.899908	-1.904106	1.106061	0.004738	0.708354
-24.755622	-2.000293	1.111066	0.004711	0.708213
-25.790240	-1.918463	1.116070	0.004904	0.708008
-25.444828	-1.975799	1.121075	0.004839	0.708016
-25.506534	-1.969993	1.126080	0.004851	0.708006
-25.859263	-1.903517	1.131085	0.004917	0.708013
-25.814543	-1.910140	1.136090	0.004908	0.708016
-25.740770	-1.926028	1.141094	0.004894	0.708010
-25.690381	-1.980571	1.146099	0.004885	0.707919
-26.872857	-1.880510	1.151104	0.005105	0.707697
-26.596722	-1.927058	1.156109	0.005054	0.707702
-26.261397	-1.987269	1.161114	0.004991	0.707701
-26.643989	-1.920802	1.166118	0.005063	0.707698
-26.670275	-1.911928	1.171123	0.005067	0.707706
-26.593705	-1.928742	1.176128	0.005053	0.707700
-26.459376	-1.955346	1.181133	0.005028	0.707695
-27.166301	-1.986026	1.186138	0.005160	0.707380
-27.508838	-1.927279	1.191142	0.005224	0.707376
-27.206868	-1.976879	1.196147	0.005167	0.707384
-27.252731	-1.973385	1.201152	0.005176	0.707375
-27.602762	-1.909842	1.206157	0.005241	0.707377
-27.630323	-1.903543	1.211162	0.005246	0.707380
-27.579315	-1.916889	1.216166	0.005237	0.707372
-27.956538	-1.979977	1.221171	0.005307	0.707110
-28.311201	-1.933724	1.226176	0.005373	0.707076
-28.490305	-1.897692	1.231181	0.005406	0.707084
-28.417759	-1.911027	1.236186	0.005393	0.707084
-28.463263	-1.904796	1.241190	0.005401	0.707080
-27.840043	-2.011155	1.246195	0.005285	0.707089
-28.370201	-1.923046	1.251200	0.005384	0.707077
-28.920410	-1.970513	1.256205	0.005486	0.706784
-28.961771	-1.980292	1.261210	0.005494	0.706750
-29.216768	-1.935047	1.266214	0.005541	0.706750
-29.345522	-1.907719	1.271219	0.005565	0.706758
-29.304621	-1.919687	1.276224	0.005558	0.706749
-29.180995	-1.938746	1.281229	0.005535	0.706755
-29.246791	-1.927110	1.286234	0.005547	0.706755
-29.922289	-1.935819	1.291238	0.005673	0.706495
-30.064281	-1.934256	1.296243	0.005699	0.706448
-30.047834	-1.940581	1.301248	0.005696	0.706441
-30.134066	-1.922078	1.306253	0.005712	0.706447
-30.040410	-1.939525	1.311258	0.005695	0.706446
-30.030220	-1.944269	1.316262	0.005693	0.706440
-30.064884	-1.933054	1.321267	0.005699	0.706450
-30.145723	-2.035437	1.326272	0.005714	0.706215
-30.857062	-1.951823	1.331277	0.005847	0.706129
-30.897659	-1.944989	1.336282	0.005854	0.706128
-31.016711	-1.926498	1.341286	0.005876	0.706122
-30.642992	-1.987502	1.346291	0.005807	0.706134
-31.039154	-1.922176	1.351296	0.005880	0.706123
-31.219835	-1.887614	1.356301	0.005914	0.706128
-31.203285	-2.010561	1.361306	0.005911	0.705887
-31.721508	-1.933020	1.366310	0.006007	0.705857
-31.928209	-1.889706	1.371315	0.006046	0.705870
-31.782122	-1.922359	1.376320	0.006019	0.705857
-31.421851	-1.982910	1.381325	0.005952	0.705864
-31.484871	-1.972001	1.386330	0.005963	0.705863
-31.732897	-1.985504	1.391334	0.006009	0.705747
-32.505242	-1.957277	1.396339	0.006153	0.705527
-32.152432	-2.024298	1.401344	0.006088	0.705519
-32.930012	-1.884143	1.406349	0.006232	0.705522
-32.522020	-1.956229	1.411354	0.006156	0.705523
-32.535104	-1.957984	1.416358	0.006159	0.705515
-32.531904	-1.953061	1.421363	0.006158	0.705526
-32.762460	-2.007498	1.426368	0.006201	0.705334
-33.538656	-1.932457	1.431373	0.006346	0.705206
-33.513457	-1.935297	1.436378	0.006341	0.705210
-33.937102	-1.862462	1.441382	0.006420	0.705204
-33.495187	-1.935209	1.446387	0.006337	0.705217
-33.321462	-1.971156	1.451392	0.006305	0.705207
-33.792004	-1.884572	1.456397	0.006393	0.705212
-33.555491	-1.984203	1.461402	0.006349	0.705096
-34.492584	-1.921650	1.466406	0.006523	0.704886
-34.217900	-1.966991	1.471411	0.006472	0.704893
-34.809838	-1.866515	1.476416	0.006582	0.704883
-34.697146	-1.884527	1.481421	0.006561	0.704887
-34.192017	-1.975523	1.486426	0.006467	0.704886
-34.861608	-1.860428	1.491430	0.006592	0.704877
-34.577825	-1.903749	1.496435	0.006539	0.704892
-35.021027	-1.975501	1.501440	0.006621	0.704588
-35.569371	-1.876828	1.506445	0.006723	0.704590
-35.739234	-1.847411	1.511450	0.006755	0.704588
-35.252444	-1.936224	1.516454	0.006664	0.704584
-35.211261	-1.939126	1.521459	0.006657	0.704593
-35.284371	-1.927307	1.526464	0.006670	0.704591
-35.123218	-1.955044	1.531469	0.006640	0.704593
-35.372890	-2.053992	1.536474	0.006687	0.704303
-36.430262	-1.887641	1.541478	0.006884	0.704259
-36.145872	-1.935686	1.546483	0.006831	0.704264
-36.075579	-1.951871	1.551488	0.006818	0.704257
-36.544551	-1.867618	1.556493	0.006905	0.704258
-36.252192	-1.919909	1.561498	0.006850	0.704258
-36.066512	-1.956473	1.566502	0.006816	0.704251
-36.877290	-1.951787	1.571507	0.006967	0.703969
-37.375026	-1.874362	1.576512	0.007059	0.703946
-37.286541	-1.889765	1.581517	0.007043	0.703947
-36.658683	-1.999009	1.586522	0.006926	0.703952
-37.259651	-1.896213	1.591526	0.007038	0.703944
-37.018421	-1.934669	1.596531	0.006993	0.703953
-36.965130	-1.948131	1.601536	0.006983	0.703945
-37.695329	-1.953490	1.606541	0.007119	0.703672
-38.120467	-1.897162	1.611546	0.007198	0.703632
-38.276152	-1.872088	1.616550	0.007227	0.703627
-37.905639	-1.934023	1.621555	0.007158	0.703635
-38.117348	-1.900778	1.626560	0.007198	0.703626
-38.039785	-1.912107	1.631565	0.007183	0.703631
-37.625587	-1.985118	1.636570	0.007106	0.703633
-38.481294	-1.927474	1.641574	0.007265	0.703441
-38.961702	-1.890476	1.646579	0.007355	0.703343
-38.623745	-1.953994	1.651584	0.007292	0.703337
-38.591737	-1.958980	1.656589	0.007286	0.703338
-38.615672	-1.953915	1.661594	0.007290	0.703340
-38.465546	-1.984292	1.666598	0.007262	0.703333
-38.210053	-2.068829	1.671603	0.007215	0.703254
-39.707644	-1.927172	1.676608	0.007494	0.703001
-39.511804	-1.961486	1.681613	0.007457	0.703002
-39.260209	-2.003848	1.686618	0.007410	0.703007
-39.734782	-1.923497	1.691622	0.007499	0.702998
-39.362834	-1.984844	1.696627	0.007429	0.703009
-39.431882	-1.976218	1.701632	0.007442	0.703001
-39.864763	-2.012218	1.706637	0.007523	0.702773
-40.667231	-1.908783	1.711642	0.007672	0.702692
-40.704259	-1.907448	1.716646	0.007679	0.702682
-40.380298	-1.957964	1.721651	0.007619	0.702697
-40.820642	-1.883596	1.726656	0.007701	0.702688
-40.778181	-1.890718	1.731661	0.007693	0.702689
-40.332281	-1.968963	1.736666	0.007610	0.702692
-40.843273	-1.944874	1.741670	0.007705	0.702556
-41.479130	-1.923487	1.746675	0.007823	0.702370
-40.904451	-2.029522	1.751680	0.007716	0.702363
-41.448399	-1.931968	1.756685	0.007817	0.702364
-41.362326	-1.943121	1.761690	0.007801	0.702373
-41.160840	-1.985007	1.766694	0.007764	0.702361
-41.155110	-1.982105	1.771699	0.007763	0.702369
-41.752851	-1.978835	1.776704	0.007874	0.702160
-42.507084	-1.890402	1.781709	0.008014	0.702067
-41.731348	-2.026462	1.786714	0.007870	0.702071
-42.391226	-1.912556	1.791718	0.007993	0.702064
-42.570261	-1.874896	1.796723	0.008026	0.702075
-42.376382	-1.913996	1.801728	0.007990	0.702066
-42.099321	-1.962063	1.806733	0.007938	0.702069
-42.527798	-1.978548	1.811738	0.008018	0.701881
-43.781657	-1.828003	1.816742	0.008252	0.701733
-43.216761	-1.923270	1.821747	0.008146	0.701745
-43.197745	-1.930956	1.826752	0.008143	0.701736
-43.180151	-1.933607	1.831757	0.008140	0.701737
-42.698961	-2.015914	1.836762	0.008050	0.701744
-43.453526	-1.887010	1.841766	0.008190	0.701733
-43.345988	-1.948354	1.846771	0.008170	0.701647
-43.770937	-1.979017	1.851776	0.008250	0.701432
-43.766005	-1.980104	1.856781	0.008249	0.701431
-44.589815	-1.829054	1.861786	0.008402	0.701440
-44.275879	-1.891410	1.866790	0.008344	0.701427
-43.681275	-1.991053	1.871795	0.008233	0.701440
-44.195707	-1.904771	1.876800	0.008329	0.701429
-44.489409	-1.881056	1.881805	0.008383	0.701371
-44.799879	-1.950622	1.886810	0.008441	0.701118
-44.897791	-1.935489	1.891814	0.008459	0.701113
-44.970073	-1.918799	1.896819	0.008473	0.701121
-44.791686	-1.951779	1.901824	0.008440	0.701119
-44.635910	-1.980188	1.906829	0.008411	0.701117
-44.738728	-1.961097	1.911834	0.008430	0.701119
-45.018635	-1.964025	1.916838	0.008482	0.701012
-45.630349	-1.922722	1.921843	0.008596	0.700875
-45.495498	-1.949711	1.926848	0.008570	0.700869
-45.821481	-1.890862	1.931853	0.008631	0.700870
-45.376561	-1.968137	1.936858	0.008548	0.700875
-45.354282	-1.977132	1.941862	0.008544	0.700864
-45.534650	-1.940128	1.946867	0.008578	0.700874
-46.027187	-2.020644	1.951872	0.008669	0.700533
-46.330549	-1.968831	1.956877	0.008726	0.700528
-46.778069	-1.886922	1.961882	0.008809	0.700533
-46.389976	-1.959494	1.966886	0.008737	0.700526
-45.933224	-2.037688	1.971891	0.008652	0.700533
-46.208727	-1.990805	1.976896	0.008703	0.700528
-46.623768	-2.021089	1.981901	0.008780	0.700317
-47.290869	-1.950438	1.986906	0.008905	0.700219
-47.300675	-1.952321	1.991910	0.008906	0.700211
-47.392178	-1.930553	1.996915	0.008923	0.700222
-47.479603	-1.919093	2.001920	0.008940	0.700214
-47.565121	-1.904025	2.011917	0.008956	0.700214
-47.868550	-1.959471	2.021914	0.009012	0.699992
-48.239327	-1.942408	2.031910	0.009081	0.699892
-48.235425	-1.945020	2.041907	0.009080	0.699888
-48.325964	-1.928747	2.051904	0.009097	0.699889
-48.233319	-1.944451	2.061901	0.009080	0.699890
-47.814441	-1.926503	2.071898	0.009002	0.700078
-47.649973	-1.888090	2.081894	0.008971	0.700216
-47.559049	-1.904796	2.091891	0.008954	0.700215
-47.401748	-1.934071	2.101888	0.008925	0.700212
-47.486090	-1.919790	2.111885	0.008941	0.700211
-47.467157	-1.922078	2.121882	0.008937	0.700213
-47.569740	-1.903234	2.131878	0.008956	0.700214
-47.425913	-1.929259	2.141875	0.008929	0.700214
-47.241790	-1.887091	2.151872	0.008895	0.700366
-46.494697	-1.941138	2.161869	0.008756	0.700526
-46.420825	-1.951950	2.171866	0.008742	0.700531
-46.611005	-1.917292	2.181862	0.008777	0.700533
-46.503617	-1.936934	2.191859	0.008757	0.700532
-46.043715	-1.905000	2.201856	0.008672	0.700763
-45.503077	-1.950492	2.211853	0.008571	0.700866
-45.614912	-1.929883	2.221850	0.008592	0.700868
-45.657461	-1.920819	2.231846	0.008600	0.700871
-45.430146	-1.908963	2.241843	0.008557	0.700977
-44.921114	-1.931091	2.251840	0.008463	0.701116
-44.991037	-1.917763	2.261837	0.008476	0.701118
-44.852108	-1.940482	2.271834	0.008450	0.701122
-44.448097	-1.888751	2.281830	0.008374	0.701373
-44.062588	-1.927491	2.291827	0.008303	0.701433
-44.094718	-1.922833	2.301824	0.008309	0.701431
-44.109739	-1.870035	2.311821	0.008311	0.701533
-43.190110	-1.931836	2.321818	0.008140	0.701740
-43.281122	-1.915404	2.331814	0.008157	0.701740
-43.181985	-1.933998	2.341811	0.008138	0.701738
-42.659885	-1.879369	2.351808	0.008041	0.702037
-42.223013	-1.941648	2.361805	0.007960	0.702069
-42.145842	-1.954548	2.371802	0.007945	0.702071
-42.189239	-1.903868	2.381798	0.007953	0.702158
-41.244100	-1.969458	2.391795	0.007778	0.702366
-41.722247	-1.884036	2.401792	0.007866	0.702366
-41.371643	-1.947083	2.411789	0.007801	0.702365
-40.970648	-1.892644	2.421786	0.007726	0.702620
-40.617164	-1.923177	2.431782	0.007661	0.702686
-40.537143	-1.936313	2.441779	0.007646	0.702688
-40.475496	-1.895118	2.451776	0.007634	0.702793
-39.388977	-1.986159	2.461773	0.007432	0.703001
-39.688173	-1.931990	2.471770	0.007488	0.703003
-39.614760	-1.944527	2.481766	0.007474	0.703004
-38.972304	-1.944669	2.491763	0.007354	0.703235
-38.970062	-1.894310	2.501760	0.007354	0.703337
-38.779545	-1.929275	2.511757	0.007318	0.703335
-38.874636	-1.880836	2.521754	0.007336	0.703399
-37.917296	-1.936158	2.531750	0.007158	0.703632
-37.845806	-1.950327	2.541747	0.007144	0.703629
-38.061246	-1.911247	2.551744	0.007184	0.703631
-37.385081	-1.914497	2.561741	0.007058	0.703867
-37.365528	-1.876710	2.571738	0.007055	0.703951
-36.974324	-1.947027	2.581734	0.006982	0.703949
-37.046320	-1.876675	2.591731	0.006995	0.704066
-36.435984	-1.891874	2.601728	0.006882	0.704254
-36.368690	-1.903551	2.611725	0.006869	0.704255
-36.290447	-1.907992	2.621722	0.006854	0.704274
-35.442304	-1.903314	2.631718	0.006696	0.704589
-35.287704	-1.933502	2.641715	0.006668	0.704583
-35.286366	-1.934235	2.651712	0.006667	0.704582
-35.026992	-1.915961	2.661709	0.006619	0.704712
-34.471577	-1.930780	2.671706	0.006516	0.704882
-34.239936	-1.970902	2.681702	0.006472	0.704884
-34.525489	-1.921265	2.691699	0.006526	0.704882
-33.806986	-1.910291	2.701696	0.006392	0.705162
-33.833416	-1.884024	2.711693	0.006397	0.705206
-33.479976	-1.945159	2.721690	0.006331	0.705209
-33.423725	-1.882109	2.731686	0.006320	0.705356
-32.847479	-1.904363	2.741683	0.006213	0.705518
-32.677350	-1.934565	2.751680	0.006181	0.705519
-32.787296	-1.907614	2.761677	0.006202	0.705534
-31.904124	-1.903707	2.771674	0.006037	0.705858
-31.692171	-1.939653	2.781670	0.005998	0.705862
-32.110513	-1.868371	2.791667	0.006076	0.705855
-31.594527	-1.888992	2.801664	0.005979	0.705999
-31.167941	-1.904700	2.811661	0.005900	0.706120
-31.047459	-1.923757	2.821658	0.005878	0.706125
-31.001981	-1.905963	2.831654	0.005869	0.706177
-30.219725	-1.914592	2.841651	0.005723	0.706440
-29.983004	-1.957906	2.851648	0.005679	0.706438
-30.226205	-1.913883	2.861645	0.005725	0.706440
-29.759374	-1.901791	2.871642	0.005638	0.706631
-29.171639	-1.946553	2.881638	0.005528	0.706752
-29.269847	-1.929348	2.891635	0.005546	0.706751
-29.183665	-1.928436	2.901632	0.005530	0.706784
-28.727443	-1.864539	2.911629	0.005445	0.707076
-28.139148	-1.966861	2.921626	0.005336	0.707081
-28.274387	-1.942939	2.931622	0.005361	0.707080
-27.947813	-1.915565	2.941619	0.005300	0.707252
-27.517499	-1.933104	2.951616	0.005220	0.707371
-27.632194	-1.912104	2.961613	0.005241	0.707372
-27.417125	-1.926983	2.971610	0.005201	0.707419
-26.826881	-1.893186	2.981606	0.005091	0.707698
-26.671388	-1.921786	2.991603	0.005062	0.707697
-26.622751	-1.931770	3.001600	0.005053	0.707694
-26.120070	-1.906863	3.011597	0.004960	0.707924
-25.646935	-1.946902	3.021594	0.004871	0.708013
-25.903120	-1.901308	3.031590	0.004919	0.708012
-25.776530	-1.893960	3.041587	0.004895	0.708073
-25.024980	-1.891855	3.051584	0.004755	0.708345
-24.738897	-1.942366	3.061581	0.004702	0.708346
-24.727844	-1.943779	3.071578	0.004700	0.708347
-24.310543	-1.921447	3.081574	0.004622	0.708541
-24.151495	-1.903356	3.091571	0.004593	0.708634
-23.883976	-1.950010	3.101568	0.004543	0.708636
-23.866388	-1.940921	3.111565	0.004540	0.708661
-23.133614	-1.924650	3.121562	0.004403	0.708955
-23.134747	-1.924632	3.131558	0.004403	0.708955
-22.997670	-1.951394	3.141555	0.004378	0.708950
-22.791864	-1.898776	3.151552	0.004339	0.709129
-22.291497	-1.921987	3.161549	0.004246	0.709261
-22.001088	-1.973890	3.171546	0.004192	0.709261
-22.447485	-1.879871	3.181542	0.004275	0.709290
-21.493341	-1.899823	3.191539	0.004097	0.709590
-21.239997	-1.944455	3.201536	0.004050	0.709591
-21.206806	-1.950164	3.211533	0.004044	0.709592
-20.880397	-1.935329	3.221530	0.003983	0.709738
-20.531815	-1.922005	3.231526	0.003918	0.709889
-20.382772	-1.947774	3.241523	0.003891	0.709890
-20.329744	-1.959676	3.251520	0.003881	0.709886
-19.725556	-1.916966	3.261517	0.003768	0.710186
-19.215988	-1.993686	3.271514	0.003673	0.710214
-19.712414	-1.905950	3.281510	0.003766	0.710213
-19.465598	-1.894425	3.291507	0.003720	0.710324
-18.767862	-1.915945	3.301504	0.003590	0.710529
-18.622657	-1.941459	3.311501	0.003563	0.710530
-18.641285	-1.939185	3.321498	0.003566	0.710528
-17.920956	-1.915732	3.331494	0.003432	0.710831
-17.363081	-1.999242	3.341491	0.003328	0.710863
-17.774517	-1.926383	3.351488	0.003405	0.710862
-17.597727	-1.942022	3.361485	0.003372	0.710894
-16.890625	-1.948632	3.371482	0.003240	0.711132
-16.813466	-1.960844	3.381478	0.003226	0.711136
-16.973473	-1.932869	3.391475	0.003255	0.711135
-16.565729	-1.897020	3.401472	0.003179	0.711351
-16.080606	-1.935307	3.411469	0.003089	0.711447
-16.263686	-1.901850	3.421466	0.003123	0.711449
-15.803961	-1.926199	3.431462	0.003037	0.711564
-15.077552	-1.959959	3.441459	0.002902	0.711755
-15.400639	-1.903632	3.451456	0.002962	0.711752
-15.242451	-1.931456	3.461453	0.002933	0.711753
-14.457036	-1.909982	3.471450	0.002787	0.712075
-14.270203	-1.937693	3.481446	0.002752	0.712086
-14.282783	-1.937206	3.491443	0.002754	0.712083
-14.406373	-1.838457	3.501440	0.002777	0.712235
-13.387094	-1.948157	3.511437	0.002587	0.712379
-13.723082	-1.887416	3.521434	0.002650	0.712381
-13.536505	-1.886358	3.531430	0.002615	0.712449
-12.818781	-1.886488	3.541427	0.002481	0.712703
-12.716220	-1.905733	3.551424	0.002462	0.712702
-12.686137	-1.910572	3.561421	0.002456	0.712703
-12.026591	-1.884736	3.571418	0.002334	0.712988
-11.685208	-1.930275	3.581414	0.002270	0.713019
-11.845320	-1.901972	3.591411	0.002300	0.713018
-11.837577	-1.833590	3.601408	0.002298	0.713157
-10.677215	-1.941522	3.611405	0.002082	0.713354
-10.944298	-1.893061	3.621402	0.002132	0.713355
-10.647818	-1.945953	3.631398	0.002077	0.713355
-10.106753	-1.922486	3.641395	0.001976	0.713594
-10.241230	-1.873282	3.651392	0.002001	0.713644
-9.873925	-1.938831	3.661389	0.001933	0.713644
-9.935249	-1.875022	3.671386	0.001944	0.713749
-8.672272	-1.990996	3.681382	0.001709	0.713966
-8.609829	-2.002700	3.691379	0.001697	0.713965
-8.712917	-1.985778	3.701376	0.001716	0.713962
-8.415898	-2.023229	3.711373	0.001661	0.713993
-7.928264	-1.970454	3.721370	0.001570	0.714270
-7.406387	-2.063499	3.731366	0.001473	0.714270
-7.802439	-1.993322	3.741363	0.001547	0.714269
-7.545010	-2.038820	3.751360	0.001499	0.714270
-6.980027	-1.983393	3.761357	0.001393	0.714580
-6.835556	-1.997705	3.771354	0.001367	0.714603
-6.621568	-2.036211	3.781350	0.001327	0.714602
-6.830404	-1.988957	3.791347	0.001366	0.714622
-5.875757	-2.018461	3.801344	0.001188	0.714901
-5.600738	-2.067091	3.811341	0.001137	0.714902
-5.827780	-2.025136	3.821338	0.001179	0.714905
-5.801305	-2.008930	3.831334	0.001174	0.714947
-5.060847	-1.999063	3.841331	0.001036	0.715228
-4.764328	-2.054397	3.851328	0.000981	0.715223
-5.075456	-1.997423	3.861325	0.001039	0.715226
-4.807421	-1.976523	3.871322	0.000989	0.715363
-3.773155	-2.071216	3.881318	0.000796	0.715540
-4.048877	-2.019210	3.891315	0.000847	0.715546
-3.985013	-2.031837	3.901312	0.000835	0.715544
-3.490704	-1.994080	3.911309	0.000743	0.715793
-2.942483	-2.047562	3.921306	0.000641	0.715881
-2.921439	-2.050314	3.931302	0.000637	0.715883
-3.079755	-2.023757	3.941299	0.000667	0.715879
-2.519294	-2.007149	3.951296	0.000562	0.716110
-2.502517	-2.000422	3.961293	0.000559	0.716130
-2.500617	-2.001854	3.971290	0.000559	0.716127
-2.058084	-1.971851	3.981286	0.000476	0.716343
-1.782387	-1.968776	3.991283	0.000425	0.716446
-1.595753	-2.002721	4.001280	0.000390	0.716445
-1.242648	-2.003557	4.011277	0.000324	0.716568
-1.069866	-1.940160	4.021274	0.000292	0.716755
-1.425434	-1.876655	4.031270	0.000358	0.716755
-1.517591	-1.766397	4.041267	0.000375	0.716941
-1.210994	-1.750845	4.051264	0.000318	0.717080
-1.233529	-1.699807	4.061261	0.000322	0.717173
-0.787566	-1.675463	4.071258	0.000239	0.717378
-0.953975	-1.622612	4.081254	0.000270	0.717424
-0.606308	-1.543359	4.091251	0.000205	0.717703
-1.099772	-1.431177	4.101248	0.000297	0.717751
-0.703038	-1.368075	4.111245	0.000223	0.718015
-0.775557	-1.283503	4.121242	0.000237	0.718157
-0.311200	-1.267828	4.131238	0.000150	0.718351
-0.392219	-1.145290	4.141235	0.000165	0.718565
-0.468316	-1.068895	4.151232	0.000179	0.718689
-0.375916	-0.949192	4.161229	0.000162	0.718958
-0.244640	-0.866592	4.171226	0.000137	0.719167
-0.351244	-0.750512	4.181222	0.000157	0.719358
-0.306913	-0.638572	4.191219	0.000149	0.719595
-0.034830	-0.541454	4.201216	0.000098	0.719882
-0.208171	-0.392010	4.211213	0.000130	0.720115
-0.268477	-0.252896	4.221210	0.000141	0.720368
-0.182797	-0.124330	4.231206	0.000125	0.720652
-0.266839	0.033445	4.241203	0.000141	0.720933
0.000000	0.142003	4.251200	0.000091	0.721240
0.019698	0.767456	4.256205	0.000087	0.722476
0.283162	1.997396	4.261210	0.000037	0.724978
0.657445	3.793462	4.266214	-0.000034	0.728614
0.706056	6.207154	4.271219	-0.000045	0.733315
0.991798	9.074378	4.276224	-0.000100	0.738938
1.328077	12.417964	4.281229	-0.000164	0.745442
1.629827	16.222680	4.286234	-0.000223	0.752748
1.842787	20.441182	4.291238	-0.000266	0.760727
2.239450	25.031947	4.296243	-0.000342	0.769369
2.620805	29.988792	4.301248	-0.000417	0.778577
2.973598	35.297552	4.306253	-0.000486	0.788302
3.539425	40.892586	4.311258	-0.000595	0.798484
3.990884	46.798359	4.316262	-0.000683	0.809047
4.567229	52.982355	4.321267	-0.000794	0.819993
4.849489	59.478434	4.326272	-0.000851	0.831238
5.399771	66.154281	4.331277	-0.000958	0.842716
6.064458	73.035931	4.336282	-0.001086	0.854414
10.183970	79.534123	4.341286	-0.001857	0.866322
11.261757	86.811148	4.346291	-0.002063	0.878460
12.318736	94.259452	4.351296	-0.002264	0.890699
13.208436	101.903885	4.356301	-0.002435	0.903033
14.213943	109.684711	4.361306	-0.002627	0.915443
15.022732	117.597156	4.366310	-0.002783	0.927835
15.621925	125.683313	4.371315	-0.002900	0.940269
16.633281	133.794350	4.376320	-0.003094	0.952686
17.803509	141.972239	4.381325	-0.003317	0.965081
18.607185	150.305186	4.386330	-0.003472	0.977450
19.437005	158.697152	4.391334	-0.003632	0.989755
20.705354	167.063774	4.396339	-0.003874	1.001981
21.267044	175.586900	4.401344	-0.003984	1.014106
21.916228	184.130142	4.406349	-0.004110	1.026136
22.975532	192.646818	4.411354	-0.004313	1.038087
24.250965	201.149875	4.416358	-0.004556	1.049933
25.220154	209.754225	4.421363	-0.004742	1.061711
26.180103	218.376182	4.426368	-0.004927	1.073381
26.770508	227.058721	4.431373	-0.005042	1.084920
27.691888	235.703578	4.436378	-0.005219	1.096362
28.479261	244.350206	4.441382	-0.005372	1.107659
29.399831	253.007326	4.446387	-0.005549	1.118883
30.134375	261.672476	4.451392	-0.005691	1.129965
30.701698	270.374354	4.456397	-0.005802	1.140950
31.578853	279.041324	4.461402	-0.005971	1.151851
33.133543	287.550021	4.466406	-0.006266	1.162598
34.265594	296.140574	4.471411	-0.006483	1.173258
34.718481	304.824116	4.476416	-0.006573	1.183794
35.517340	313.445616	4.481421	-0.006727	1.194233
36.548452	321.999618	4.486426	-0.006925	1.204548
36.932175	330.658215	4.491430	-0.007002	1.214768
37.533010	339.269717	4.496435	-0.007119	1.224891
38.143405	347.880149	4.501440	-0.007239	1.234932
38.625387	356.452773	4.506445	-0.007334	1.244824
39.306654	364.998967	4.511450	-0.007467	1.254645
40.045209	373.492286	4.516454	-0.007610	1.264341
40.772290	382.012318	4.521459	-0.007751	1.273991
41.584123	390.479889	4.526464	-0.007907	1.283526
41.994198	399.012986	4.531469	-0.007989	1.292988
42.504823	407.519730	4.536474	-0.008090	1.302371
43.332266	416.024805	4.541478	-0.008249	1.311742
44.588684	424.431946	4.546483	-0.008489	1.321018
45.391766	432.829640	4.551488	-0.008644	1.330138
46.320200	441.207723	4.556493	-0.008822	1.339197
46.818860	449.653006	4.561498	-0.008921	1.348190
47.305689	458.081675	4.566502	-0.009017	1.357103
48.291979	466.410113	4.571507	-0.009206	1.365941
48.806336	474.841134	4.576512	-0.009307	1.374746
49.278475	483.233053	4.581517	-0.009401	1.383448
50.269877	491.571861	4.586522	-0.009591	1.392128
50.760953	499.943211	4.591526	-0.009687	1.400704
51.219292	508.324589	4.596531	-0.009778	1.409232
51.866265	516.666935	4.601536	-0.009904	1.417700
52.354724	525.006850	4.606541	-0.010001	1.426089
53.038333	533.336639	4.611546	-0.010133	1.434451
53.436265	541.665858	4.616550	-0.010213	1.442718
54.166252	549.963732	4.621555	-0.010354	1.450960
54.619805	558.301927	4.626560	-0.010444	1.459150
55.152529	566.602393	4.631565	-0.010549	1.467270
56.369340	574.866562	4.636570	-0.010781	1.475419
56.825907	583.152871	4.641574	-0.010871	1.483424
57.385652	591.448676	4.646579	-0.010981	1.491411
57.788061	599.756969	4.651584	-0.011061	1.499343
58.495514	607.997121	4.656589	-0.011198	1.507216
58.853686	616.316882	4.661594	-0.011270	1.515068
59.250758	624.578505	4.666598	-0.011350	1.522832
59.880778	632.828961	4.671603	-0.011472	1.530582
60.528319	641.065151	4.676608	-0.011598	1.538281
60.941614	649.313470	4.681613	-0.011681	1.545918
61.590217	657.587810	4.686618	-0.011807	1.553576
62.373217	665.771271	4.691622	-0.011958	1.561133
62.967190	674.008118	4.696627	-0.012074	1.568674
63.216106	682.298835	4.701632	-0.012126	1.576177
63.541263	690.545386	4.706637	-0.012192	1.583617
64.193011	698.764205	4.711642	-0.012318	1.591043
64.586636	706.993438	4.716646	-0.012397	1.598407
65.106015	715.199522	4.721651	-0.012499	1.605734
65.439240	723.453146	4.726656	-0.012567	1.613044
65.788171	731.669077	4.731661	-0.012637	1.620290
66.402355	739.860245	4.736666	-0.012757	1.627518
67.494503	748.036177	4.741670	-0.012965	1.634768
67.971471	756.235429	4.746675	-0.013060	1.641920
68.468707	764.426334	4.751680	-0.013157	1.649037
68.910161	772.647126	4.756685	-0.013245	1.656141
69.188635	780.871533	4.761690	-0.013302	1.663196
69.712767	789.048200	4.766694	-0.013405	1.670213
70.329024	797.231018	4.771699	-0.013525	1.677219
70.848717	805.397946	4.776704	-0.013627	1.684168
71.010958	813.627215	4.781709	-0.013663	1.691094
71.558182	821.802853	4.786714	-0.013770	1.697998
72.071770	829.951336	4.791718	-0.013871	1.704846
72.413568	838.174761	4.796723	-0.013940	1.711707
72.976520	846.329131	4.801728	-0.014050	1.718511
73.319747	854.481165	4.806733	-0.014120	1.725259
73.584517	862.704362	4.811738	-0.014174	1.732028
74.016012	870.853193	4.816742	-0.014260	1.738731
74.552443	878.994613	4.821747	-0.014365	1.745416
75.319609	887.125171	4.826752	-0.014513	1.752096
76.063096	895.246655	4.831757	-0.014657	1.758739
76.660682	903.389681	4.836762	-0.014774	1.765357
77.080962	911.572751	4.841766	-0.014857	1.771959
77.417966	919.766409	4.846771	-0.014925	1.778535
77.691165	927.937095	4.851776	-0.014982	1.785060
78.148469	936.122053	4.856781	-0.015072	1.791596
78.526661	944.312758	4.861786	-0.015148	1.798102
78.748909	952.441059	4.866790	-0.015195	1.804517
78.973490	960.617739	4.871795	-0.015242	1.810947
79.494537	968.740279	4.876800	-0.015344	1.817348
79.742268	976.883846	4.881805	-0.015395	1.823710
80.262888	985.023575	4.886810	-0.015498	1.830079
80.368635	993.198069	4.891814	-0.015523	1.836404
80.901158	1001.295897	4.896819	-0.015627	1.842698
81.454803	1009.405237	4.901824	-0.015736	1.848982
82.206437	1017.504596	4.906829	-0.015881	1.855260
82.408656	1025.677991	4.911834	-0.015924	1.861509
82.749376	1033.816706	4.916838	-0.015993	1.867727
83.395937	1041.967824	4.921843	-0.016118	1.873969
83.680887	1050.091744	4.926848	-0.016177	1.880127
84.087700	1058.199905	4.931853	-0.016258	1.886268
84.441842	1066.360626	4.936858	-0.016329	1.892422
84.916266	1074.455870	4.941862	-0.016423	1.898521
85.461053	1082.562302	4.946867	-0.016529	1.904616
85.578933	1090.745103	4.951872	-0.016557	1.910700
86.045287	1098.848144	4.956877	-0.016649	1.916745
86.370452	1106.975408	4.961882	-0.016715	1.922773
86.795402	1115.077907	4.966886	-0.016799	1.928775
87.112300	1123.228290	4.971891	-0.016863	1.934781
87.641234	1131.318671	4.976896	-0.016967	1.940748
87.793871	1139.475507	4.981901	-0.017001	1.946704
88.463492	1147.601015	4.986906	-0.017131	1.952675
88.698816	1155.728497	4.991910	-0.017180	1.958583
89.161415	1163.805990	4.996915	-0.017271	1.964460
89.840995	1171.866532	5.001920	-0.017403	1.970332
90.362859	1179.971110	5.006925	-0.017506	1.976200
90.801922	1188.086784	5.011930	-0.017593	1.982050
91.075639	1196.197714	5.016934	-0.017649	1.987861
91.441691	1204.342435	5.021939	-0.017723	1.993690
92.005436	1212.412267	5.026944	-0.017833	1.999469
92.119684	1220.545593	5.031949	-0.017859	2.005229
92.566025	1228.661011	5.036954	-0.017948	2.010994
92.975046	1236.765358	5.041958	-0.018029	2.016731
93.308572	1244.874836	5.046963	-0.018097	2.022448
93.590307	1252.994605	5.051968	-0.018154	2.028150
94.060579	1261.125412	5.056973	-0.018247	2.033863
94.564521	1269.200507	5.061978	-0.018346	2.039525
94.982681	1277.268648	5.066982	-0.018430	2.045157
95.425676	1285.384022	5.071987	-0.018517	2.050809
96.159278	1293.444422	5.076992	-0.018659	2.056437
96.487457	1301.539499	5.081997	-0.018726	2.062032
96.875358	1309.656330	5.087002	-0.018803	2.067633
97.379833	1317.749438	5.092006	-0.018902	2.073214
98.112164	1325.804509	5.097011	-0.019044	2.078777
98.331611	1333.920963	5.102016	-0.019090	2.084315
98.679842	1342.013045	5.107021	-0.019160	2.089835
99.194428	1350.134806	5.112026	-0.019261	2.095377
99.331847	1358.242281	5.117030	-0.019292	2.100857
99.540989	1366.370664	5.122035	-0.019337	2.106345
99.975271	1374.501400	5.127040	-0.019423	2.111841
100.201230	1382.624866	5.132045	-0.019470	2.117298
100.798035	1390.648577	5.137050	-0.019586	2.122710
101.237438	1398.712369	5.142054	-0.019674	2.128119
101.868797	1406.783093	5.147059	-0.019796	2.133538
102.104877	1414.900417	5.152064	-0.019846	2.138936
102.498016	1422.950388	5.157069	-0.019924	2.144291
103.226200	1431.005567	5.162074	-0.020065	2.149668
103.484901	1439.123383	5.167078	-0.020118	2.155027
103.797639	1447.217671	5.172083	-0.020182	2.160363
104.273705	1455.283606	5.177088	-0.020276	2.165683
104.633956	1463.381199	5.182093	-0.020348	2.170999
105.017519	1471.502336	5.187098	-0.020425	2.176320
105.334170	1479.565997	5.192102	-0.020489	2.181584
106.087221	1487.614062	5.197107	-0.020635	2.186866
106.342085	1495.755827	5.202112	-0.020687	2.192149
106.738521	1503.836799	5.207117	-0.020767	2.197393
107.168914	1511.903662	5.212122	-0.020852	2.202619
107.582178	1519.970985	5.217126	-0.020934	2.207831
108.153879	1528.050522	5.222131	-0.021046	2.213053
108.469631	1536.137330	5.227136	-0.021110	2.218244
108.821520	1544.207822	5.232141	-0.021181	2.223415
109.283550	1552.288817	5.237146	-0.021272	2.228591
109.534717	1560.401704	5.242150	-0.021324	2.233757
109.858862	1568.470483	5.247155	-0.021390	2.238889
110.328247	1576.532791	5.252160	-0.021482	2.244017
110.448402	1584.641975	5.257165	-0.021510	2.249133
110.750172	1592.742946	5.262170	-0.021572	2.254248
111.152841	1600.792911	5.267174	-0.021652	2.259328
111.417310	1608.873729	5.272179	-0.021706	2.264404
111.652951	1616.966605	5.277184	-0.021756	2.269474
112.357004	1625.071409	5.282189	-0.021892	2.274580
112.523180	1633.145493	5.287194	-0.021928	2.279609
112.520040	1641.224596	5.292198	-0.021933	2.284615
113.007018	1649.243513	5.297203	-0.022029	2.289616
113.339182	1657.345436	5.302208	-0.022096	2.294643
113.486669	1665.398106	5.307213	-0.022129	2.299613
113.978596	1673.455378	5.312218	-0.022226	2.304604
114.154326	1681.534038	5.317222	-0.022264	2.309571
114.448613	1689.634179	5.322227	-0.022324	2.314550
115.334952	1697.608341	5.327232	-0.022494	2.319492
115.837638	1705.645552	5.332237	-0.022593	2.324428
116.458231	1713.716023	5.337242	-0.022714	2.329385
116.862465	1721.812946	5.342246	-0.022794	2.334328
117.266463	1729.883455	5.347251	-0.022875	2.339245
117.590464	1737.965267	5.352256	-0.022940	2.344152
117.963148	1746.041831	5.357261	-0.023015	2.349050
118.596836	1754.139703	5.362266	-0.023138	2.353971
118.888111	1762.185341	5.367270	-0.023198	2.358823
119.132364	1770.259834	5.372275	-0.023248	2.363678
119.340952	1778.340743	5.377280	-0.023293	2.368524
119.778890	1786.422440	5.382285	-0.023379	2.373379
120.099147	1794.500039	5.387290	-0.023444	2.378212
120.132978	1802.569831	5.392294	-0.023456	2.383008
120.633774	1810.623169	5.397299	-0.023554	2.387822
120.983661	1818.704562	5.402304	-0.023625	2.392630
121.347369	1826.759056	5.407309	-0.023698	2.397414
121.769966	1834.800292	5.412314	-0.023782	2.402185
121.947986	1842.864586	5.417318	-0.023820	2.406941
122.445510	1850.913402	5.422323	-0.023918	2.411703
122.941811	1858.978361	5.427328	-0.024016	2.416465
123.106235	1867.046347	5.432333	-0.024052	2.421194
123.642663	1875.098936	5.437338	-0.024157	2.425933
123.841739	1883.202819	5.442342	-0.024199	2.430667
124.253315	1891.308853	5.447347	-0.024281	2.435409
124.601888	1899.346318	5.452352	-0.024351	2.440097
124.630795	1907.389705	5.457357	-0.024362	2.444755
125.022166	1915.452772	5.462362	-0.024440	2.449443
125.217361	1923.516365	5.467366	-0.024482	2.454108
125.492720	1931.577335	5.472371	-0.024538	2.458768
125.618438	1939.648331	5.477376	-0.024567	2.463414
126.001465	1947.673531	5.482381	-0.024643	2.468044
126.407019	1955.756167	5.487386	-0.024724	2.472700
126.802010	1963.780458	5.492390	-0.024803	2.477313
127.219171	1971.810233	5.497395	-0.024886	2.481922
127.501241	1979.873567	5.502400	-0.024944	2.486531
127.740472	1987.949627	5.507405	-0.024994	2.491136
128.079043	1996.041715	5.512410	-0.025062	2.495749
128.373862	2004.070445	5.517414	-0.025122	2.500314
128.697955	2012.118563	5.522419	-0.025188	2.504884
128.956135	2020.196179	5.527424	-0.025241	2.509457
129.333533	2028.287804	5.532429	-0.025317	2.514039
129.972190	2036.302200	5.537434	-0.025441	2.518587
130.162876	2044.344357	5.542438	-0.025481	2.523111
130.540009	2052.403160	5.547443	-0.025557	2.527649
130.892389	2060.460841	5.552448	-0.025628	2.532176
131.222322	2068.517267	5.557453	-0.025694	2.536693
131.656138	2076.564083	5.562458	-0.025781	2.541204
131.841976	2084.621608	5.567462	-0.025820	2.545695
132.209908	2092.704427	5.572467	-0.025894	2.550205
132.556702	2100.775132	5.577472	-0.025964	2.554699
132.622608	2108.820105	5.582477	-0.025982	2.559151
133.179278	2116.834341	5.587482	-0.026090	2.563612
133.404640	2124.894230	5.592486	-0.026138	2.568068
133.748714	2132.956137	5.597491	-0.026207	2.572525
134.073982	2141.027784	5.602496	-0.026273	2.576979
133.978606	2149.104320	5.607501	-0.026260	2.581398
134.528326	2157.131687	5.612506	-0.026368	2.585828
134.759764	2165.215042	5.617510	-0.026416	2.590258
135.013696	2173.462028	5.622515	-0.026469	2.594772
135.327855	2181.429238	5.627520	-0.026533	2.599129
135.434149	2189.413509	5.632525	-0.026558	2.603475
135.694912	2197.452731	5.637530	-0.026612	2.607853
135.885605	2205.496740	5.642534	-0.026652	2.612222
136.297150	2213.510743	5.647539	-0.026734	2.616582
137.076973	2221.499676	5.652544	-0.026885	2.620945
137.389563	2229.518454	5.657549	-0.026948	2.625287
137.611176	2237.613058	5.662554	-0.026995	2.629655
138.048109	2245.671434	5.667558	-0.027081	2.634012
138.298382	2253.717447	5.672563	-0.027133	2.638342
138.642898	2261.765249	5.677568	-0.027202	2.642672
138.863397	2269.800170	5.682573	-0.027249	2.646980
139.482033	2277.845796	5.687578	-0.027369	2.651312
139.495910	2285.939356	5.692582	-0.027377	2.655624
139.686812	2293.990966	5.697587	-0.027418	2.659918
140.130797	2302.014244	5.702592	-0.027506	2.664206
140.662983	2310.028776	5.707597	-0.027610	2.668488
141.034183	2318.117410	5.712602	-0.027685	2.672792
141.193890	2326.189384	5.717606	-0.027720	2.677066
141.694298	2334.185093	5.722611	-0.027818	2.681316
141.813853	2342.257664	5.727616	-0.027846	2.685574
142.259842	2350.266258	5.732621	-0.027934	2.689813
142.581165	2358.364689	5.737626	-0.027999	2.694085
142.814953	2366.412786	5.742630	-0.028048	2.698318
143.102827	2374.445667	5.747635	-0.028107	2.702539
143.575071	2382.486500	5.752640	-0.028200	2.706770
143.994525	2390.520166	5.757645	-0.028283	2.710987
144.255713	2398.625117	5.762650	-0.028337	2.715224
144.453892	2406.629644	5.767654	-0.028379	2.719399
144.723596	2414.678384	5.772659	-0.028435	2.723595
145.011526	2422.732707	5.777664	-0.028494	2.727788
145.126407	2430.793602	5.782669	-0.028520	2.731967
145.699901	2438.847569	5.787674	-0.028632	2.736165
145.955069	2446.872627	5.792678	-0.028685	2.740322
146.227104	2454.880134	5.797683	-0.028741	2.744464
146.845459	2462.927645	5.802688	-0.028861	2.748641
147.102689	2471.037014	5.807693	-0.028914	2.752822
147.337651	2479.127372	5.812698	-0.028964	2.756986
147.594362	2487.119559	5.817702	-0.029017	2.761094
148.035173	2495.132762	5.822707	-0.029104	2.765218
148.370277	2503.171173	5.827712	-0.029172	2.769342
148.392719	2511.261373	5.832717	-0.029181	2.773468
148.509830	2519.313926	5.837722	-0.029208	2.777574
148.819099	2527.323507	5.842726	-0.029271	2.781663
149.159119	2535.342096	5.847731	-0.029339	2.785753
149.404208	2543.391087	5.852736	-0.029390	2.789847
149.739239	2551.442855	5.857741	-0.029458	2.793941
149.987310	2559.500617	5.862746	-0.029509	2.798027
150.393747	2567.503092	5.867750	-0.029590	2.802089
151.075127	2575.508031	5.872755	-0.029722	2.806161
151.459066	2583.561093	5.877760	-0.029799	2.810235
151.590327	2591.650127	5.882765	-0.029829	2.814306
151.980521	2599.686369	5.887770	-0.029907	2.818359
152.336432	2607.704650	5.892774	-0.029978	2.822396
152.421861	2615.770540	5.897779	-0.029999	2.826435
152.641529	2623.840832	5.902784	-0.030046	2.830479
153.041234	2631.880355	5.907789	-0.030125	2.834511
153.556801	2639.890146	5.912794	-0.030227	2.838529
153.642940	2647.955318	5.917798	-0.030248	2.842545
153.869074	2655.989659	5.922803	-0.030295	2.846548
154.145949	2664.032848	5.927808	-0.030352	2.850552
154.510729	2672.065589	5.932813	-0.030425	2.854551
154.869573	2680.110471	5.937818	-0.030497	2.858549
155.211216	2688.125737	5.942822	-0.030566	2.862526
155.211228	2696.198342	5.947827	-0.030571	2.866507
155.526720	2704.256298	5.952832	-0.030635	2.870493
155.763202	2712.290647	5.957837	-0.030685	2.874457
155.982851	2720.310113	5.962842	-0.030731	2.878407
156.305998	2728.351469	5.967846	-0.030796	2.882368
156.791426	2736.364301	5.972851	-0.030892	2.886319
157.193970	2744.416126	5.977856	-0.030972	2.890278
157.259576	2752.483362	5.982861	-0.030990	2.894222
157.677902	2760.513586	5.987866	-0.031073	2.898161
158.152892	2768.529457	5.992870	-0.031166	2.902090
158.264214	2776.596617	5.997875	-0.031192	2.906020
158.395219	2784.661661	6.002880	-0.031222	2.909944
158.677087	2792.779036	6.007885	-0.031280	2.913897
158.963012	2800.781383	6.012890	-0.031338	2.917788
159.286167	2808.779514	6.017894	-0.031404	2.921675
159.724992	2816.768700	6.022899	-0.031491	2.925557
160.259093	2824.771283	6.027904	-0.031595	2.929447
160.126063	2832.883490	6.032909	-0.031576	2.933348
160.325560	2840.919590	6.037914	-0.031618	2.937225
160.484043	2848.966978	6.042918	-0.031653	2.941101
160.795950	2856.952445	6.047923	-0.031716	2.944949
161.034664	2865.004040	6.052928	-0.031766	2.948820
161.246050	2873.056251	6.057933	-0.031811	2.952686
161.653359	2881.094072	6.062938	-0.031892	2.956549
161.751041	2889.124933	6.067942	-0.031915	2.960387
162.088475	2897.133950	6.072947	-0.031983	2.964223
162.572960	2905.169241	6.077952	-0.032079	2.968074
162.495126	2913.241300	6.082957	-0.032070	2.971908
162.851551	2921.314816	6.087962	-0.032141	2.975761
163.012848	2929.332870	6.092966	-0.032176	2.979572
163.407849	2937.331768	6.097971	-0.032255	2.983380
163.566954	2945.399867	6.102976	-0.032290	2.987205
163.756614	2953.450689	6.107981	-0.032331	2.991018
164.131810	2961.512760	6.112986	-0.032406	2.994841
164.496200	2969.492347	6.117990	-0.032479	2.998620
164.794147	2977.503147	6.122995	-0.032540	3.002405
165.321253	2985.524668	6.128000	-0.032643	3.006202
165.600660	2993.532752	6.133005	-0.032700	3.009975
165.844124	3001.619440	6.138010	-0.032751	3.013778
166.252972	3009.640445	6.143014	-0.032832	3.017554
166.559549	3017.693101	6.148019	-0.032895	3.021336
166.678164	3025.738845	6.153024	-0.032922	3.025099
167.167408	3033.746691	6.158029	-0.033018	3.028859
167.454608	3041.830010	6.163034	-0.033077	3.032639
167.661233	3049.876886	6.168038	-0.033121	3.036394
167.655663	3057.901374	6.173043	-0.033125	3.040123
168.050045	3065.927340	6.178048	-0.033204	3.043867
168.306350	3073.949351	6.183053	-0.033257	3.047599
168.520350	3082.022123	6.188058	-0.033302	3.051347
168.664428	3090.060791	6.193062	-0.033334	3.055072
168.880668	3098.085038	6.198067	-0.033379	3.058788
169.361205	3106.095478	6.203072	-0.033474	3.062507
169.569439	3114.116628	6.208077	-0.033518	3.066212
169.854975	3122.185186	6.213082	-0.033577	3.069939
169.944044	3130.319051	6.218086	-0.033598	3.073682
170.095949	3138.325854	6.223091	-0.033632	3.077365
170.499063	3146.327067	6.228096	-0.033712	3.081053
170.644562	3154.289136	6.233101	-0.033745	3.084706
171.030039	3162.321833	6.238106	-0.033822	3.088399
171.416102	3170.351982	6.243110	-0.033899	3.092085
171.626103	3178.388423	6.248115	-0.033943	3.095763
172.137336	3186.401526	6.253120	-0.034043	3.099438
172.608552	3194.395486	6.258125	-0.034136	3.103099
172.928967	3202.465063	6.263130	-0.034201	3.106783
172.942322	3210.528289	6.268134	-0.034209	3.110446
173.162822	3218.577628	6.273139	-0.034255	3.114107
173.761589	3226.574105	6.278144	-0.034372	3.117758
173.880652	3234.618926	6.283149	-0.034400	3.121404
173.984039	3242.655424	6.288154	-0.034424	3.125041
174.207383	3250.697091	6.293158	-0.034471	3.128682
174.626890	3258.737885	6.298163	-0.034554	3.132327
174.941937	3266.780527	6.303168	-0.034618	3.135964
175.021231	3274.784338	6.308173	-0.034638	3.139569
175.290287	3282.819784	6.313178	-0.034694	3.143192
175.532408	3290.848493	6.318182	-0.034744	3.146806
175.909615	3298.852458	6.323187	-0.034819	3.150412
176.201385	3306.955033	6.328192	-0.034879	3.154053
176.344343	3314.965692	6.333197	-0.034911	3.157643
176.660233	3322.996011	6.338202	-0.034975	3.161245
176.844420	3331.005028	6.343206	-0.035014	3.164827
176.953699	3339.034671	6.348211	-0.035040	3.168412
177.204838	3347.129219	6.353216	-0.035092	3.172027
177.423109	3355.111995	6.358221	-0.035138	3.175587
177.695822	3363.157667	6.363226	-0.035194	3.179173
177.930806	3371.174659	6.368230	-0.035243	3.182741
178.021194	3379.204756	6.373235	-0.035265	3.186304
178.612048	3387.227800	6.378240	-0.035380	3.189882
178.750445	3395.272945	6.383245	-0.035411	3.193446
179.091291	3403.336164	6.388250	-0.035480	3.197023
179.497600	3411.337953	6.393254	-0.035561	3.200571
180.008003	3419.318410	6.398259	-0.035661	3.204110
180.321063	3427.386216	6.403264	-0.035725	3.207675
180.334538	3435.422553	6.408269	-0.035733	3.211210
180.677964	3443.467244	6.413274	-0.035802	3.214759
181.016972	3451.509316	6.418278	-0.035870	3.218302
181.033519	3459.528685	6.423283	-0.035878	3.221818
181.471310	3467.525233	6.428288	-0.035965	3.225337
181.727483	3475.584845	6.433293	-0.036018	3.228873
181.997025	3483.675772	6.438298	-0.036074	3.232419
182.262669	3491.746741	6.443302	-0.036128	3.235952
182.234014	3499.682746	6.448307	-0.036128	3.239411
182.743044	3507.700059	6.453312	-0.036228	3.242923
182.954162	3515.731606	6.458317	-0.036273	3.246425
183.275978	3523.734406	6.463322	-0.036338	3.249915
183.515365	3531.788106	6.468326	-0.036388	3.253421
183.420906	3539.849592	6.473331	-0.036375	3.256912
183.972056	3547.831649	6.478336	-0.036483	3.260391
184.302209	3555.862219	6.483341	-0.036550	3.263879
184.453388	3563.915720	6.488346	-0.036583	3.267366
184.787967	3571.939490	6.493350	-0.036651	3.270843
185.344950	3579.950302	6.498355	-0.036760	3.274320
185.625051	3587.988498	6.503360	-0.036817	3.277793
185.751290	3596.007917	6.508365	-0.036846	3.281249
185.785360	3604.047091	6.513370	-0.036858	3.284707
186.255292	3612.059841	6.518374	-0.036950	3.288166
186.567153	3620.103488	6.523379	-0.037014	3.291629
186.884659	3628.177125	6.528384	-0.037078	3.295101
186.888558	3636.191199	6.533389	-0.037084	3.298531
187.328324	3644.195866	6.538394	-0.037171	3.301971
187.642218	3652.227634	6.543398	-0.037235	3.305414
187.924922	3660.233377	6.548403	-0.037293	3.308841
188.182540	3668.344316	6.553408	-0.037346	3.312308
188.196593	3676.368825	6.558413	-0.037354	3.315726
188.445774	3684.360289	6.563418	-0.037406	3.319135
188.704895	3692.374655	6.568422	-0.037459	3.322550
188.865004	3700.384036	6.573427	-0.037494	3.325957
189.186308	3708.424389	6.578432	-0.037559	3.329378
189.375926	3716.457428	6.583437	-0.037600	3.332788
189.434164	3724.541274	6.588442	-0.037616	3.336212
189.498103	3732.545777	6.593446	-0.037633	3.339598
189.864144	3740.540294	6.598451	-0.037706	3.342988
190.201707	3748.572232	6.603456	-0.037774	3.346389
190.259252	3756.599709	6.608461	-0.037790	3.349775
190.689213	3764.647668	6.613466	-0.037876	3.353179
191.041781	3772.685444	6.618470	-0.037947	3.356572
191.138110	3780.665111	6.623475	-0.037970	3.359929
191.572425	3788.715326	6.628480	-0.038056	3.363324
192.053874	3796.738569	6.633485	-0.038151	3.366706
192.393219	3804.759142	6.638490	-0.038219	3.370078
192.443626	3812.846136	6.643494	-0.038234	3.373464
192.582945	3820.852285	6.648499	-0.038265	3.376816
192.973265	3828.871340	6.653504	-0.038343	3.380179
193.274373	3836.873186	6.658509	-0.038404	3.383528
193.528802	3844.922274	6.663514	-0.038457	3.386892
193.899496	3852.934438	6.668518	-0.038531	3.390241
193.800440	3861.052020	6.673523	-0.038518	3.393615
194.245505	3869.099679	6.678528	-0.038606	3.396975
194.603601	3877.021354	6.683533	-0.038678	3.400276
195.042707	3885.035266	6.688538	-0.038765	3.403615
195.248171	3893.072953	6.693542	-0.038809	3.406952
195.184941	3901.063230	6.698547	-0.038802	3.410257
195.629811	3909.129391	6.703552	-0.038890	3.413608
195.424750	3917.196208	6.708557	-0.038857	3.416934
195.803906	3925.167339	6.713562	-0.038933	3.420237
196.026613	3933.192572	6.718566	-0.038980	3.423553
196.033881	3941.235808	6.723571	-0.038986	3.426867
196.348864	3949.259350	6.728576	-0.039050	3.430179
196.723584	3957.300357	6.733581	-0.039125	3.433497
196.863006	3965.329726	6.738586	-0.039156	3.436800
197.328945	3973.326627	6.743590	-0.039248	3.440097
197.079187	3981.330832	6.748595	-0.039207	3.443369
197.496366	3989.389225	6.753600	-0.039290	3.446683
197.649878	3997.419614	6.758605	-0.039324	3.449974
198.049293	4005.448635	6.763610	-0.039404	3.453269
198.257902	4013.504678	6.768614	-0.039448	3.456566
198.498892	4021.508496	6.773619	-0.039498	3.459839
198.591871	4029.543347	6.778624	-0.039520	3.463116
198.771041	4037.559806	6.783629	-0.039559	3.466386
199.089499	4045.597410	6.788634	-0.039623	3.469666
199.149354	4053.687131	6.793638	-0.039640	3.472956
199.572727	4061.671146	6.798643	-0.039724	3.476211
199.802346	4069.678926	6.803648	-0.039772	3.479467
200.000311	4077.673691	6.808653	-0.039814	3.482713
200.089784	4085.710773	6.813658	-0.039836	3.485970
200.629487	4093.714707	6.818662	-0.039942	3.489225
200.896891	4101.743034	6.823667	-0.039997	3.492478
201.225195	4109.800529	6.828672	-0.040063	3.495741
201.336506	4117.781160	6.833677	-0.040089	3.498964
201.769642	4125.793826	6.838682	-0.040175	3.502206
202.096658	4133.815360	6.843686	-0.040241	3.505446
202.125133	4141.869865	6.848691	-0.040252	3.508686
202.504569	4149.921893	6.853696	-0.040328	3.511934
202.760308	4157.929604	6.858701	-0.040380	3.515157
202.816822	4165.937479	6.863706	-0.040396	3.518371
203.334447	4173.995390	6.868710	-0.040498	3.521616
203.417977	4181.986430	6.873715	-0.040519	3.524818
203.835726	4190.024165	6.878720	-0.040602	3.528045
203.936484	4198.066941	6.883725	-0.040626	3.531263
204.220931	4206.102420	6.888730	-0.040684	3.534479
204.532910	4214.138581	6.893734	-0.040747	3.537695
204.516434	4222.146587	6.898739	-0.040749	3.540886
204.968835	4230.168178	6.903744	-0.040839	3.544093
205.242801	4238.211401	6.908749	-0.040895	3.547301
205.369047	4246.243997	6.913754	-0.040924	3.550497
205.741009	4254.380428	6.918758	-0.040998	3.553739
205.729201	4262.349865	6.923763	-0.041001	3.556900
206.164555	4270.338951	6.928768	-0.041088	3.560080
206.401543	4278.318501	6.933773	-0.041137	3.563247
206.738322	4286.350009	6.938778	-0.041205	3.566434
206.878357	4294.372515	6.943782	-0.041236	3.569610
206.837455	4302.409181	6.948787	-0.041234	3.572783
207.296129	4310.442555	6.953792	-0.041325	3.575966
207.608601	4318.442474	6.958797	-0.041388	3.579129
207.661851	4326.462135	6.963802	-0.041403	3.582289
207.946205	4334.475313	6.968806	-0.041461	3.585451
208.097107	4342.476762	6.973811	-0.041495	3.588601
208.213434	4350.588787	6.978816	-0.041522	3.591791
208.459223	4358.576215	6.983821	-0.041573	3.594933
208.815049	4366.558867	6.988826	-0.041644	3.598074
208.970474	4374.607650	6.993830	-0.041678	3.601232
208.987314	4382.580917	6.998835	-0.041687	3.604353
209.504179	4390.627724	7.003840	-0.041788	3.607515
209.559944	4398.643437	7.008845	-0.041804	3.610649
209.539784	4406.723522	7.013850	-0.041805	3.613803
209.694657	4414.787894	7.018854	-0.041839	3.616953
209.904410	4422.730495	7.023859	-0.041884	3.620055
210.384397	4430.752465	7.028864	-0.041978	3.623192
210.404313	4438.808212	7.033869	-0.041987	3.626326
210.562748	4446.828330	7.038874	-0.042022	3.629448
210.995606	4454.886982	7.043878	-0.042108	3.632590
211.201523	4462.896136	7.048883	-0.042151	3.635704
211.449577	4470.932698	7.053888	-0.042203	3.638826
211.637787	4478.944939	7.058893	-0.042243	3.641935
211.908452	4486.928583	7.063898	-0.042299	3.645032
212.325466	4494.959170	7.068902	-0.042382	3.648149
212.658255	4502.951661	7.073907	-0.042449	3.651246
212.745593	4511.037429	7.078912	-0.042470	3.654370
212.832862	4519.071866	7.083917	-0.042492	3.657471
213.031470	4527.088592	7.088922	-0.042534	3.660566
213.325799	4535.100041	7.093926	-0.042594	3.663659
213.351092	4543.105709	7.098931	-0.042604	3.666740
213.599297	4551.173812	7.103936	-0.042656	3.669848
213.982182	4559.191044	7.108941	-0.042732	3.672937
214.321935	4567.181466	7.113946	-0.042801	3.676012
214.207796	4575.210648	7.118950	-0.042785	3.679088
214.470360	4583.210849	7.123955	-0.042839	3.682160
214.841854	4591.248977	7.128960	-0.042913	3.685246
214.826849	4599.248532	7.133965	-0.042916	3.688305
215.076207	4607.309218	7.138970	-0.042967	3.691392
215.564032	4615.359457	7.143974	-0.043063	3.694478
215.737151	4623.345589	7.148979	-0.043101	3.697529
215.960526	4631.367071	7.153984	-0.043148	3.700593
216.338848	4639.348308	7.158989	-0.043223	3.703642
216.720396	4647.396001	7.163994	-0.043300	3.706714
217.094669	4655.441161	7.168998	-0.043375	3.709782
217.162905	4663.512916	7.174003	-0.043393	3.712850
217.412399	4671.579718	7.179008	-0.043444	3.715919
217.467048	4679.551349	7.184013	-0.043460	3.718944
217.905212	4687.561004	7.189018	-0.043547	3.721990
218.238857	4695.514803	7.194022	-0.043614	3.725010
218.342090	4703.535266	7.199027	-0.043638	3.728047
218.378673	4711.601247	7.204032	-0.043650	3.731097
218.734774	4719.636292	7.209037	-0.043722	3.734141
219.046620	4727.612989	7.214042	-0.043785	3.737159
219.129368	4735.647939	7.219046	-0.043806	3.740191
219.179646	4743.678223	7.224051	-0.043820	3.743218
219.567939	4751.684811	7.229056	-0.043898	3.746242
219.741258	4759.711424	7.234061	-0.043936	3.749265
219.734773	4767.784004	7.239066	-0.043940	3.752299
220.117902	4775.814082	7.244070	-0.044016	3.755324
220.220572	4783.793198	7.249075	-0.044041	3.758321
220.434613	4791.846852	7.254080	-0.044086	3.761346
220.525613	4799.799593	7.259085	-0.044108	3.764328
220.700049	4807.843690	7.264090	-0.044146	3.767343
220.881441	4815.891388	7.269094	-0.044185	3.770358
221.068457	4823.911849	7.274099	-0.044225	3.773360
221.320987	4831.994199	7.279104	-0.044277	3.776384
221.601853	4839.945018	7.284109	-0.044334	3.779358
221.635703	4847.975702	7.289114	-0.044346	3.782353
221.885320	4855.999850	7.294118	-0.044398	3.785348
222.069207	4864.023488	7.299123	-0.044437	3.788340
222.424241	4872.108861	7.304128	-0.044509	3.791355
222.577063	4880.130479	7.309133	-0.044542	3.794340
222.848306	4888.113646	7.314138	-0.044598	3.797311
223.098528	4896.106953	7.319142	-0.044650	3.800283
223.116939	4904.110138	7.324147	-0.044658	3.803251
223.450478	4912.139077	7.329152	-0.044726	3.806233
223.635098	4920.162907	7.334157	-0.044765	3.809208
223.821883	4928.166798	7.339162	-0.044805	3.812173
224.231691	4936.224075	7.344166	-0.044887	3.815160
224.339075	4944.211458	7.349171	-0.044912	3.818112
224.426241	4952.271401	7.354176	-0.044934	3.821089
224.479878	4960.232887	7.359181	-0.044949	3.824026
224.812127	4968.278676	7.364186	-0.045016	3.826998
224.976668	4976.298014	7.369190	-0.045052	3.829954
225.242118	4984.356946	7.374195	-0.045107	3.832925
225.657666	4992.353443	7.379200	-0.045189	3.835873
225.822188	5000.348327	7.384205	-0.045225	3.838813
225.789082	5008.407322	7.389210	-0.045224	3.841771
226.189796	5016.368184	7.394214	-0.045304	3.844699
226.392867	5024.419612	7.399219	-0.045347	3.847654
226.515920	5032.421222	7.404224	-0.045375	3.850587
226.589703	5040.494881	7.409229	-0.045394	3.853543
226.957428	5048.509862	7.414234	-0.045468	3.856481
227.122697	5056.545679	7.419238	-0.045504	3.859420
227.175248	5064.593026	7.424243	-0.045519	3.862359
227.413675	5072.565320	7.429248	-0.045569	3.865272
227.581354	5080.631553	7.434253	-0.045605	3.868216
227.867462	5088.626420	7.439258	-0.045664	3.871134
228.057153	5096.900382	7.444262	-0.045704	3.874149
228.204396	5104.861994	7.449267	-0.045737	3.877048
228.375120	5112.791420	7.454272	-0.045774	3.879933
228.455150	5120.749736	7.459277	-0.045794	3.882824
228.731626	5128.712169	7.464282	-0.045851	3.885719
229.116694	5136.742085	7.469286	-0.045928	3.888638
229.104732	5144.777651	7.474291	-0.045931	3.891549
229.462450	5152.829954	7.479296	-0.046003	3.894471
229.607950	5160.847808	7.484301	-0.046035	3.897375
229.772489	5168.792961	7.489306	-0.046071	3.900250
230.026982	5176.853490	7.494310	-0.046123	3.903167
230.150954	5184.876757	7.499315	-0.046152	3.906065
230.369324	5192.898565	7.504320	-0.046198	3.908963
230.548344	5200.920655	7.509325	-0.046236	3.911858
230.832930	5208.953758	7.514330	-0.046294	3.914756
231.014976	5216.964342	7.519334	-0.046334	3.917642
231.239473	5224.942281	7.524339	-0.046381	3.920515
231.460738	5232.960234	7.529344	-0.046427	3.923401
231.894957	5240.974299	7.534349	-0.046513	3.926286
231.847077	5248.995222	7.539354	-0.046509	3.929164
231.999659	5257.055509	7.544358	-0.046543	3.932057
232.282213	5265.063012	7.549363	-0.046601	3.934931
232.455900	5273.111573	7.554368	-0.046639	3.937815
232.606547	5281.103534	7.559373	-0.046672	3.940677
232.927105	5289.091240	7.564378	-0.046737	3.943539
233.016794	5297.171427	7.569382	-0.046759	3.946427
233.011456	5305.148500	7.574387	-0.046763	3.949274
233.438972	5313.191641	7.579392	-0.046848	3.952151
233.524319	5321.254828	7.584397	-0.046869	3.955027
233.701322	5329.231813	7.589402	-0.046907	3.957871
234.010362	5337.231945	7.594406	-0.046970	3.960724
234.102158	5345.226460	7.599411	-0.046992	3.963569
234.331244	5353.278196	7.604416	-0.047040	3.966435
234.514741	5361.248337	7.609421	-0.047080	3.969269
234.707325	5369.287185	7.614426	-0.047121	3.972125
234.902248	5377.353815	7.619430	-0.047162	3.974989
235.023655	5385.369003	7.624435	-0.047190	3.977832
235.326074	5393.374450	7.629440	-0.047252	3.980672
235.635818	5401.360698	7.634445	-0.047314	3.983503
235.841940	5409.363760	7.639450	-0.047358	3.986337
236.084901	5417.455751	7.644454	-0.047409	3.989200
236.341007	5425.437202	7.649459	-0.047462	3.992023
236.604572	5433.547983	7.654464	-0.047516	3.994889
236.645573	5441.564159	7.659469	-0.047529	3.997716
237.200350	5449.520130	7.664474	-0.047637	4.000529
237.421686	5457.540496	7.669478	-0.047684	4.003356
237.444507	5465.556055	7.674483	-0.047693	4.006177
237.768184	5473.573548	7.679488	-0.047759	4.009001
238.253685	5481.621606	7.684493	-0.047854	4.011837
238.356025	5489.627684	7.689498	-0.047879	4.014649
238.554353	5497.679680	7.694502	-0.047921	4.017477
238.956538	5505.654519	7.699507	-0.048001	4.020280
239.337616	5513.693966	7.704512	-0.048077	4.023102
239.267067	5521.739341	7.709517	-0.048069	4.025918
239.470627	5529.756084	7.714522	-0.048112	4.028726
239.888296	5537.775490	7.719526	-0.048195	4.031536
239.755351	5545.893249	7.724531	-0.048176	4.034370
240.198640	5553.906057	7.729536	-0.048264	4.037174
240.459581	5561.838429	7.734541	-0.048318	4.039946
240.633575	5569.814103	7.739546	-0.048355	4.042729
240.854917	5577.832789	7.744550	-0.048402	4.045526
241.032457	5585.835648	7.749555	-0.048440	4.048315
241.573312	5593.899780	7.754560	-0.048546	4.051129
241.744253	5601.939386	7.759565	-0.048583	4.053926
242.027548	5609.929617	7.764570	-0.048641	4.056706
242.018304	5617.937556	7.769574	-0.048644	4.059486
242.152164	5625.935195	7.774579	-0.048675	4.062263
242.236794	5633.963806	7.779584	-0.048696	4.065048
242.503119	5641.989653	7.784589	-0.048750	4.067832
242.580565	5649.989999	7.789594	-0.048770	4.070604
242.850536	5658.052145	7.794598	-0.048826	4.073397
242.952893	5666.030939	7.799603	-0.048850	4.076157
243.481255	5673.989109	7.804608	-0.048953	4.078914
243.440344	5682.099468	7.809613	-0.048951	4.081714
243.397722	5690.085119	7.814618	-0.048948	4.084469
243.842926	5698.119415	7.819622	-0.049037	4.087245
243.933260	5706.075402	7.824627	-0.049059	4.089988
244.202212	5714.144078	7.829632	-0.049114	4.092770
244.461791	5722.188778	7.834637	-0.049168	4.095542
244.853686	5730.146743	7.839642	-0.049246	4.098283
245.150515	5738.207471	7.844646	-0.049306	4.101057
245.300534	5746.206647	7.849651	-0.049339	4.103806
245.596599	5754.223899	7.854656	-0.049400	4.106561
245.655216	5762.259298	7.859661	-0.049416	4.109318
245.693585	5770.346452	7.864666	-0.049428	4.112090
245.985279	5778.392206	7.869670	-0.049488	4.114849
246.341934	5786.373541	7.874675	-0.049560	4.117585
246.383579	5794.325450	7.879680	-0.049573	4.120305
246.581704	5802.382861	7.884685	-0.049615	4.123062
246.958007	5810.387097	7.889690	-0.049690	4.125800
246.859587	5818.431524	7.894694	-0.049677	4.128545
246.933951	5826.443870	7.899699	-0.049696	4.131279
247.210773	5834.479904	7.904704	-0.049753	4.134021
247.440140	5842.525851	7.909709	-0.049801	4.136765
247.434317	5850.499406	7.914714	-0.049805	4.139479
247.739825	5858.558023	7.919718	-0.049867	4.142224
248.125973	5866.488826	7.924723	-0.049944	4.144925
248.404635	5874.552842	7.929728	-0.050001	4.147668
248.731578	5882.587517	7.934733	-0.050067	4.150400
248.938302	5890.613395	7.939738	-0.050111	4.153126
249.128448	5898.645211	7.944742	-0.050152	4.155851
249.294151	5906.602116	7.949747	-0.050188	4.158549
249.636735	5914.636617	7.954752	-0.050257	4.161274
249.890625	5922.622325	7.959757	-0.050309	4.163979
250.053460	5930.680134	7.964762	-0.050345	4.166706
250.166085	5938.696927	7.969766	-0.050371	4.169416
250.510482	5946.692762	7.974771	-0.050441	4.172120
250.466835	5954.753999	7.979776	-0.050438	4.174841
250.596751	5962.808278	7.984781	-0.050467	4.177559
250.787044	5970.723196	7.989786	-0.050508	4.180229
250.924803	5978.804439	7.994790	-0.050539	4.182952
251.046823	5986.786689	7.999795	-0.050567	4.185641
251.534409	5994.778135	8.004800	-0.050663	4.188334
251.481593	6002.876767	8.009805	-0.050658	4.191056
251.519854	6010.957303	8.014810	-0.050670	4.193772
251.902825	6018.987551	8.019814	-0.050747	4.196472
252.257303	6026.872317	8.024819	-0.050818	4.199121
252.254870	6034.932622	8.029824	-0.050823	4.201824
252.510722	6042.911823	8.034829	-0.050876	4.204500
252.827287	6050.887819	8.039834	-0.050940	4.207175
253.119332	6058.930434	8.044838	-0.051000	4.209869
252.980033	6066.992397	8.049843	-0.050979	4.212564
253.308118	6075.015433	8.054848	-0.051045	4.215249
253.331560	6083.033249	8.059853	-0.051055	4.217927
253.391086	6090.981192	8.064858	-0.051071	4.220581
253.810584	6099.032081	8.069862	-0.051155	4.223271
253.919519	6107.025306	8.074867	-0.051180	4.225937
254.256037	6115.063833	8.079872	-0.051248	4.228618
254.108065	6123.111383	8.084877	-0.051226	4.231296
254.510973	6131.118968	8.089882	-0.051306	4.233965
254.846837	6139.187232	8.094886	-0.051374	4.236651
254.621242	6147.129222	8.099891	-0.051337	4.239288
254.942303	6155.190366	8.104896	-0.051402	4.241968
255.321566	6163.127142	8.109901	-0.051478	4.244606
255.645067	6171.194856	8.114906	-0.051543	4.247285
255.813272	6179.177895	8.119910	-0.051580	4.249933
256.085222	6187.243265	8.124915	-0.051636	4.252607
256.019113	6195.247603	8.129920	-0.051629	4.255257
256.116815	6203.336473	8.134925	-0.051652	4.257934
256.340140	6211.267475	8.139930	-0.051699	4.260558
256.652364	6219.360809	8.144934	-0.051762	4.263235
256.555737	6227.289592	8.149939	-0.051750	4.265853
256.910449	6235.399627	8.154944	-0.051821	4.268532
257.144493	6243.404441	8.159949	-0.051870	4.271174
257.262329	6251.474181	8.164954	-0.051897	4.273835
257.518912	6259.506558	8.169958	-0.051950	4.276483
257.862293	6267.395713	8.174963	-0.052019	4.279083
257.966099	6275.462009	8.179968	-0.052044	4.281738
258.066335	6283.455565	8.184973	-0.052068	4.284367
258.181971	6291.487909	8.189978	-0.052094	4.287007
258.527262	6299.497690	8.194982	-0.052164	4.289640
258.656184	6307.566396	8.199987	-0.052193	4.292289
258.762937	6315.569272	8.204992	-0.052218	4.294915
259.095690	6323.598303	8.209997	-0.052285	4.297549
259.230055	6331.579010	8.215002	-0.052316	4.300165
259.281381	6339.594281	8.220006	-0.052330	4.302789
259.610716	6347.611723	8.225011	-0.052397	4.305415
259.786121	6355.611063	8.230016	-0.052435	4.308032
260.059419	6363.673281	8.235021	-0.052491	4.310668
260.256945	6371.684921	8.240026	-0.052533	4.313286
260.533276	6379.711197	8.245030	-0.052590	4.315907
260.474655	6387.694525	8.250035	-0.052584	4.318511
260.654691	6395.695499	8.255040	-0.052623	4.321120
260.935191	6403.668475	8.260045	-0.052680	4.323720
261.022460	6411.759026	8.265050	-0.052702	4.326354
261.216994	6419.757185	8.270054	-0.052743	4.328958
261.130145	6427.774027	8.275059	-0.052732	4.331564
261.407125	6435.824371	8.280064	-0.052789	4.334182
261.640311	6443.879674	8.285069	-0.052838	4.336800
261.477255	6451.790512	8.290074	-0.052813	4.339367
261.880813	6459.859719	8.295078	-0.052893	4.341987
261.994263	6467.820528	8.300083	-0.052919	4.344569
262.237754	6475.873099	8.305088	-0.052970	4.347179
262.528758	6483.898788	8.310093	-0.053029	4.349780
262.660510	6491.975071	8.315098	-0.053059	4.352394
262.856996	6500.066569	8.320102	-0.053101	4.355012
263.023833	6507.983891	8.325107	-0.053137	4.357572
263.426621	6515.966109	8.330112	-0.053218	4.360153
263.618035	6523.987301	8.335117	-0.053258	4.362744
263.705182	6531.933065	8.340122	-0.053280	4.365308
264.004831	6540.011237	8.345126	-0.053341	4.367915
264.198182	6548.025610	8.350131	-0.053382	4.370498
264.123431	6556.021665	8.355136	-0.053373	4.373073
264.570894	6564.091412	8.360141	-0.053462	4.375673
264.661223	6572.086229	8.365146	-0.053484	4.378245
264.845458	6580.115189	8.370150	-0.053524	4.380828
264.890606	6588.106729	8.375155	-0.053537	4.383395
265.053198	6596.076600	8.380160	-0.053573	4.385956
265.241379	6604.138338	8.385165	-0.053613	4.388544
265.515111	6612.158656	8.390170	-0.053669	4.391117
265.908361	6620.223660	8.395174	-0.053748	4.393705
265.898468	6628.244790	8.400179	-0.053751	4.396274
265.968639	6636.190273	8.405184	-0.053769	4.398818
266.381136	6644.257752	8.410189	-0.053852	4.401402
266.583818	6652.195845	8.415194	-0.053894	4.403941
266.577538	6660.292441	8.420198	-0.053899	4.406529
266.713267	6668.257602	8.425203	-0.053929	4.409073
267.177813	6676.312290	8.430208	-0.054021	4.411647
267.444102	6684.325991	8.435213	-0.054076	4.414205
267.475921	6692.383289	8.440218	-0.054087	4.416774
267.622240	6700.369092	8.445222	-0.054119	4.419319
267.710701	6708.403572	8.450227	-0.054141	4.421878
267.670423	6716.385765	8.455232	-0.054139	4.424419
268.047330	6724.434243	8.460237	-0.054214	4.426981
268.071673	6732.426756	8.465242	-0.054224	4.429522
268.251453	6740.516047	8.470246	-0.054263	4.432092
268.451612	6748.493781	8.475251	-0.054305	4.434627
268.721943	6756.520471	8.480256	-0.054361	4.437175
269.039801	6764.486266	8.485261	-0.054425	4.439703
269.079739	6772.558947	8.490266	-0.054438	4.442262
269.253530	6780.510348	8.495270	-0.054475	4.444782
269.327679	6788.577105	8.500275	-0.054495	4.447336
269.602254	6796.566052	8.505280	-0.054551	4.449865
269.917294	6804.618401	8.510285	-0.054615	4.452413
270.135708	6812.620368	8.515290	-0.054661	4.454943
270.146339	6820.653224	8.520294	-0.054668	4.457481
270.264388	6828.602342	8.525299	-0.054695	4.459991
270.545962	6836.635230	8.530304	-0.054753	4.462527
270.687779	6844.657584	8.535309	-0.054784	4.465057
270.610087	6852.670200	8.540314	-0.054775	4.467582
270.824428	6860.735622	8.545318	-0.054820	4.470123
270.917137	6868.761428	8.550323	-0.054843	4.472650
271.123445	6876.748908	8.555328	-0.054887	4.475164
271.409119	6884.777867	8.560333	-0.054945	4.477690
271.682748	6892.738074	8.565338	-0.055001	4.480193
271.927250	6900.733964	8.570343	-0.055052	4.482705
271.748789	6908.764532	8.575347	-0.055024	4.485225
272.126666	6916.798089	8.580352	-0.055099	4.487747
272.426683	6924.816155	8.585357	-0.055161	4.490262
272.405007	6932.842862	8.590362	-0.055162	4.492777
272.672476	6940.901317	8.595367	-0.055217	4.495302
272.986510	6948.904140	8.600371	-0.055281	4.497808
272.818445	6956.898837	8.605376	-0.055254	4.500309
273.139605	6964.901696	8.610381	-0.055320	4.502812
273.233966	6972.852094	8.615386	-0.055342	4.505297
273.616365	6980.918539	8.620391	-0.055419	4.507817
273.684211	6988.952167	8.625395	-0.055437	4.510325
273.870839	6996.993375	8.630400	-0.055477	4.512834
274.337525	7005.043008	8.635405	-0.055569	4.515345
274.174270	7012.980750	8.640410	-0.055544	4.517819
274.555530	7021.028126	8.645415	-0.055620	4.520326
274.842082	7029.008563	8.650419	-0.055678	4.522811
274.883545	7036.960059	8.655424	-0.055691	4.525285
275.038936	7045.048748	8.660429	-0.055726	4.527800
275.517420	7053.013294	8.665434	-0.055820	4.530276
275.648008	7061.115288	8.670439	-0.055849	4.532793
275.887613	7069.110517	8.675443	-0.055899	4.535275
276.028640	7077.133961	8.680448	-0.055931	4.537764
276.320618	7085.135836	8.685453	-0.055990	4.540246
276.528718	7093.120503	8.690458	-0.056034	4.542721
276.747507	7101.134763	8.695463	-0.056080	4.545204
276.831538	7109.214716	8.700467	-0.056101	4.547705
276.870816	7117.131822	8.705472	-0.056114	4.550154
277.148728	7125.237917	8.710477	-0.056171	4.552661
277.375912	7133.241715	8.715482	-0.056218	4.555135
277.536949	7141.296755	8.720487	-0.056254	4.557624
277.481075	7149.250948	8.725491	-0.056248	4.560079
277.637994	7157.314849	8.730496	-0.056283	4.562567
278.016224	7165.269985	8.735501	-0.056359	4.565021
277.871392	7173.318551	8.740506	-0.056337	4.567501
278.118209	7181.326537	8.745511	-0.056388	4.569968
278.466935	7189.380221	8.750515	-0.056458	4.572448
278.801681	7197.371479	8.755520	-0.056526	4.574907
278.927417	7205.429697	8.760525	-0.056554	4.577385
279.113438	7213.360102	8.765530	-0.056594	4.579823
279.368727	7221.417652	8.770535	-0.056647	4.582299
279.327249	7229.413184	8.775539	-0.056645	4.584753
279.437509	7237.492069	8.780544	-0.056670	4.587233
279.805630	7245.476147	8.785549	-0.056744	4.589682
279.839613	7253.498793	8.790554	-0.056756	4.592141
280.085544	7261.558082	8.795559	-0.056807	4.594610
280.170999	7269.567950	8.800563	-0.056828	4.597063
280.470423	7277.508451	8.805568	-0.056889	4.599493
280.546007	7285.584142	8.810573	-0.056908	4.601963
280.767694	7293.496589	8.815578	-0.056955	4.604382
281.051120	7301.576794	8.820583	-0.057013	4.606851
280.947614	7309.592004	8.825587	-0.056999	4.609298
281.215041	7317.617567	8.830592	-0.057054	4.611748
281.654441	7325.655726	8.835597	-0.057141	4.614200
281.672259	7333.656196	8.840602	-0.057149	4.616639
281.680852	7341.657833	8.845607	-0.057156	4.619077
281.757501	7349.721178	8.850611	-0.057176	4.621533
281.952634	7357.667906	8.855616	-0.057217	4.623952
281.988984	7365.702866	8.860621	-0.057229	4.626397
282.215057	7373.679704	8.865626	-0.057277	4.628822
282.682820	7381.773190	8.870631	-0.057369	4.631282
282.507978	7389.758004	8.875635	-0.057342	4.633707
282.547317	7397.799810	8.880640	-0.057354	4.636148
282.897099	7405.776549	8.885645	-0.057425	4.638569
283.084968	7413.755165	8.890650	-0.057465	4.640988
283.262056	7421.804966	8.895655	-0.057503	4.643428
283.135334	7429.836612	8.900659	-0.057485	4.645861
283.460234	7437.856198	8.905664	-0.057550	4.648289
283.674324	7445.850877	8.910669	-0.057595	4.650709
283.789089	7453.877360	8.915674	-0.057622	4.653136
283.900522	7461.920471	8.920679	-0.057648	4.655568
284.133015	7469.904203	8.925683	-0.057697	4.657980
284.103967	7477.896333	8.930688	-0.057696	4.660393
284.267870	7485.970979	8.935693	-0.057732	4.662830
284.389992	7493.908964	8.940698	-0.057760	4.665225
284.379824	7501.986168	8.945703	-0.057763	4.667660
284.593751	7509.982628	8.950707	-0.057809	4.670070
284.894701	7518.033493	8.955712	-0.057870	4.672495
284.857924	7526.093191	8.960717	-0.057868	4.674921
284.835989	7534.036757	8.965722	-0.057869	4.677311
285.019632	7542.024957	8.970727	-0.057909	4.679713
285.455048	7550.079010	8.975731	-0.057995	4.682133
285.684924	7558.002123	8.980736	-0.058043	4.684513
286.102027	7566.108325	8.985741	-0.058126	4.686947
285.960760	7574.036475	8.990746	-0.058105	4.689326
286.259777	7582.123416	8.995751	-0.058166	4.691751
286.569079	7590.153278	9.000755	-0.058229	4.694158
286.801406	7598.154558	9.005760	-0.058277	4.696555
286.777723	7606.163451	9.010765	-0.058278	4.698954
286.945407	7614.138165	9.015770	-0.058314	4.701341
287.159415	7622.193540	9.020775	-0.058360	4.703750
287.244359	7630.207254	9.025779	-0.058381	4.706146
287.335369	7638.209468	9.030784	-0.058403	4.708538
287.690336	7646.261798	9.035789	-0.058474	4.710942
287.779650	7654.261835	9.040794	-0.058496	4.713331
287.898169	7662.316445	9.045799	-0.058523	4.715734
288.040503	7670.303179	9.050803	-0.058555	4.718116
288.383456	7678.254908	9.055808	-0.058624	4.720485
288.773644	7686.326483	9.060813	-0.058702	4.722889
288.757815	7694.344096	9.065818	-0.058704	4.725277
288.934770	7702.342383	9.070823	-0.058743	4.727657
289.157935	7710.378806	9.075827	-0.058789	4.730047
289.347101	7718.368648	9.080832	-0.058830	4.732423
289.629330	7726.439160	9.085837	-0.058888	4.734820
289.690779	7734.399162	9.090842	-0.058904	4.737185
289.935553	7742.407132	9.095847	-0.058955	4.739561
289.928259	7750.463935	9.100851	-0.058959	4.741952
290.062249	7758.402079	9.105856	-0.058989	4.744306
290.153673	7766.488079	9.110861	-0.059011	4.746703
290.495278	7774.495609	9.115866	-0.059080	4.749074
290.510597	7782.543675	9.120871	-0.059088	4.751458
290.680934	7790.583857	9.125875	-0.059125	4.753837
290.515136	7798.574611	9.130880	-0.059100	4.756202
290.816622	7806.562152	9.135885	-0.059161	4.758563
291.187288	7814.530314	9.140890	-0.059235	4.760916
291.402595	7822.551410	9.145895	-0.059281	4.763285
291.606972	7830.581741	9.150899	-0.059324	4.765655
291.962131	7838.578908	9.155904	-0.059395	4.768014
292.158815	7846.651198	9.160909	-0.059437	4.770394
292.101420	7854.658620	9.165914	-0.059432	4.772755
292.376346	7862.652130	9.170919	-0.059488	4.775109
292.389985	7870.686485	9.175923	-0.059496	4.777475
292.542362	7878.625944	9.180928	-0.059529	4.779812
292.711959	7886.742595	9.185933	-0.059566	4.782199
292.780397	7894.636836	9.190938	-0.059584	4.784520
293.002525	7902.767671	9.195943	-0.059631	4.786909
293.252374	7910.725546	9.200947	-0.059683	4.789246
293.415932	7918.748897	9.205952	-0.059718	4.791601
294.023848	7926.807307	9.210957	-0.059837	4.793964
293.957225	7934.823637	9.215962	-0.059830	4.796316
294.206991	7942.790104	9.220967	-0.059881	4.798650
294.563283	7950.815471	9.225971	-0.059953	4.801001
294.628460	7958.780681	9.230976	-0.059970	4.803333
295.126060	7966.875008	9.235981	-0.060068	4.805701
295.447894	7974.857599	9.240986	-0.060133	4.808035
295.542583	7982.849074	9.245991	-0.060156	4.810372
295.497587	7990.412768	9.250995	-0.060153	4.812583
295.821527	7995.038773	9.256000	-0.060216	4.813933
296.278401	7997.755249	9.261005	-0.060303	4.814725
296.241352	7999.051035	9.266010	-0.060297	4.815104
296.382822	7999.515104	9.271015	-0.060324	4.815238
296.403810	8000.359849	9.276019	-0.060328	4.815485
296.502773	8000.423487	9.281024	-0.060347	4.815503
296.593895	8000.399346	9.286029	-0.060364	4.815496
296.844425	8000.497564	9.291034	-0.060410	4.815523
297.017787	8000.382861	9.296039	-0.060443	4.815489
296.955228	8000.449166	9.301043	-0.060431	4.815508
296.847127	8000.465546	9.306048	-0.060411	4.815514
297.110887	8000.399374	9.311053	-0.060460	4.815493
297.043447	8000.437806	9.316058	-0.060447	4.815505
297.270445	8000.395609	9.321063	-0.060490	4.815491
297.387315	8000.530094	9.326067	-0.060511	4.815530
297.301366	8000.535083	9.331072	-0.060496	4.815532
297.312266	8000.414478	9.336077	-0.060497	4.815497
297.349775	8000.431135	9.341082	-0.060504	4.815501
297.400177	8000.424490	9.346087	-0.060514	4.815499
297.331506	8000.537726	9.351091	-0.060501	4.815532
297.410664	8000.541178	9.356096	-0.060516	4.815533
297.728831	8000.379706	9.361101	-0.060575	4.815484
297.613844	8000.537069	9.366106	-0.060554	4.815531
297.582298	8000.395450	9.371111	-0.060548	4.815490
297.669850	8000.418282	9.376115	-0.060564	4.815496
297.994615	8000.497427	9.381120	-0.060625	4.815518
297.954293	8000.423003	9.386125	-0.060617	4.815496
297.765465	8000.554556	9.391130	-0.060582	4.815535
298.075593	8000.421811	9.396135	-0.060640	4.815495
297.872353	8000.509300	9.401139	-0.060602	4.815522
297.879556	8000.554316	9.406144	-0.060603	4.815535
298.097014	8000.438204	9.411149	-0.060644	4.815500
298.066512	8000.544593	9.416154	-0.060638	4.815531
298.105309	8000.537756	9.421159	-0.060645	4.815529
298.071514	8000.529714	9.426163	-0.060639	4.815527
297.984022	8000.548573	9.431168	-0.060623	4.815532
298.043607	8000.365707	9.436173	-0.060634	4.815479
297.933505	8000.422673	9.441178	-0.060613	4.815496
298.111709	8000.541075	9.446183	-0.060647	4.815530
298.109231	8000.515381	9.451187	-0.060646	4.815522
298.064366	8000.638635	9.456192	-0.060638	4.815558
298.204614	8000.523380	9.461197	-0.060664	4.815524
298.172892	8000.409548	9.466202	-0.060658	4.815491
298.215121	8000.529971	9.471207	-0.060666	4.815526
298.280450	8000.382474	9.476211	-0.060678	4.815483
298.462689	8000.643115	9.481216	-0.060712	4.815558
298.470887	8000.433738	9.486221	-0.060714	4.815497
298.364344	8000.551693	9.491226	-0.060694	4.815532
298.586031	8000.365102	9.496231	-0.060735	4.815476
298.538524	8000.427382	9.501235	-0.060726	4.815494
298.415884	8000.406108	9.506240	-0.060703	4.815489
298.510513	8000.442954	9.511245	-0.060721	4.815499
298.559829	8000.379637	9.516250	-0.060730	4.815480
298.489261	8000.548430	9.521255	-0.060717	4.815530
298.512878	8000.335035	9.526259	-0.060722	4.815468
298.490131	8000.471483	9.531264	-0.060717	4.815508
298.583689	8000.424934	9.536269	-0.060735	4.815493
298.639091	8000.374546	9.541274	-0.060745	4.815478
298.704533	8000.180018	9.546279	-0.060757	4.815421
298.434551	8000.413912	9.551283	-0.060707	4.815491
298.249316	8000.499561	9.556288	-0.060673	4.815517
298.566644	8000.547587	9.561293	-0.060732	4.815529
298.749115	8000.532444	9.566298	-0.060766	4.815524
298.717864	8000.426101	9.571303	-0.060760	4.815493
298.640792	8000.357480	9.576307	-0.060746	4.815473
298.782837	8000.425044	9.581312	-0.060772	4.815493
298.691937	8000.437433	9.586317	-0.060755	4.815497
298.585360	8000.550043	9.591322	-0.060735	4.815530
298.730478	8000.428455	9.596327	-0.060762	4.815494
298.800721	8000.433898	9.601331	-0.060775	4.815495
298.750310	8000.457648	9.606336	-0.060766	4.815502
298.933918	8000.409387	9.611341	-0.060800	4.815487
298.872534	8000.394473	9.616346	-0.060789	4.815483
298.791555	8000.371752	9.621351	-0.060774	4.815477
298.775180	8000.296656	9.626355	-0.060771	4.815455
298.828853	8000.365960	9.631360	-0.060781	4.815475
298.798089	8000.382554	9.636365	-0.060775	4.815480
298.901277	8000.518955	9.641370	-0.060794	4.815519
299.080791	8000.412903	9.646375	-0.060828	4.815488
299.116114	8000.395318	9.651379	-0.060834	4.815482
298.939693	8000.537769	9.656384	-0.060802	4.815525
298.919336	8000.342884	9.661389	-0.060798	4.815468
299.092747	8000.431279	9.666394	-0.060830	4.815493
299.129440	8000.381648	9.671399	-0.060837	4.815478
298.956061	8000.515598	9.676403	-0.060805	4.815518
299.057003	8000.425345	9.681408	-0.060823	4.815491
299.062514	8000.182787	9.686413	-0.060824	4.815420
298.865970	8000.348420	9.691418	-0.060788	4.815470
298.888341	8000.423619	9.696423	-0.060792	4.815492
298.914424	8000.433673	9.701427	-0.060797	4.815494
298.966842	8000.337270	9.706432	-0.060807	4.815466
299.179776	8000.286289	9.711437	-0.060846	4.815450
299.078700	8000.398990	9.716442	-0.060828	4.815483
299.106535	8000.208112	9.721447	-0.060833	4.815428
298.941524	8000.421302	9.726451	-0.060802	4.815491
299.094590	8000.341535	9.731456	-0.060830	4.815467
299.234891	8000.136489	9.736461	-0.060856	4.815406
299.068054	8000.422337	9.741466	-0.060826	4.815490
299.262942	8000.227817	9.746471	-0.060862	4.815433
299.120539	8000.321661	9.751475	-0.060835	4.815461
299.139916	8000.271743	9.756480	-0.060839	4.815446
299.156576	8000.339365	9.761485	-0.060842	4.815466
299.121987	8000.340930	9.766490	-0.060836	4.815466
299.219902	8000.224972	9.771495	-0.060854	4.815432
299.140090	8000.168064	9.776499	-0.060839	4.815416
299.183235	8000.303468	9.781504	-0.060847	4.815455
299.242472	8000.249936	9.786509	-0.060858	4.815439
299.197794	8000.312264	9.791514	-0.060850	4.815458
299.085203	8000.301845	9.796519	-0.060829	4.815455
299.092118	8000.264548	9.801523	-0.060830	4.815444
298.990102	8000.391130	9.806528	-0.060811	4.815482
298.943186	8000.381801	9.811533	-0.060803	4.815479
298.903025	8000.381136	9.816538	-0.060795	4.815479
299.003526	8000.379598	9.821543	-0.060814	4.815478
299.012383	8000.371195	9.826547	-0.060815	4.815476
299.024743	8000.439815	9.831552	-0.060818	4.815496
299.052454	8000.388966	9.836557	-0.060823	4.815481
299.252964	8000.452157	9.841562	-0.060860	4.815498
299.283994	8000.336157	9.846567	-0.060866	4.815464
299.346064	8000.266638	9.851571	-0.060878	4.815444
299.154228	8000.434488	9.856576	-0.060842	4.815493
299.171254	8000.277636	9.861581	-0.060845	4.815448
299.263821	8000.417068	9.866586	-0.060862	4.815488
299.332654	8000.241834	9.871591	-0.060875	4.815436
299.139736	8000.389356	9.876595	-0.060839	4.815480
299.159046	8000.508332	9.881600	-0.060843	4.815515
299.387503	8000.371023	9.886605	-0.060885	4.815474
299.308181	8000.540742	9.891610	-0.060871	4.815524
299.418304	8000.335192	9.896615	-0.060891	4.815463
299.364146	8000.313985	9.901619	-0.060881	4.815457
299.293575	8000.364125	9.906624	-0.060868	4.815472
299.303577	8000.275569	9.911629	-0.060870	4.815446
299.294328	8000.267934	9.916634	-0.060868	4.815444
299.578150	8000.255542	9.921639	-0.060921	4.815439
299.578815	8000.402002	9.926643	-0.060921	4.815482
299.296263	8000.455037	9.931648	-0.060869	4.815499
299.501181	8000.403923	9.936653	-0.060907	4.815483
299.388945	8000.299442	9.941658	-0.060886	4.815453
299.281252	8000.356448	9.946663	-0.060866	4.815470
299.429203	8000.263768	9.951667	-0.060893	4.815442
299.431166	8000.286250	9.956672	-0.060894	4.815449
299.418897	8000.198394	9.961677	-0.060891	4.815423
299.549158	8000.436797	9.966682	-0.060916	4.815492
299.452872	8000.423441	9.971687	-0.060898	4.815489
299.478270	8000.172659	9.976691	-0.060903	4.815415
299.384002	8000.428714	9.981696	-0.060885	4.815491
299.705110	8000.257667	9.986701	-0.060945	4.815439
299.726624	8000.375611	9.991706	-0.060949	4.815473
299.326646	8000.325146	9.996711	-0.060874	4.815461
299.619035	8000.260518	10.001715	-0.060929	4.815440
299.583283	8000.497236	10.006720	-0.060922	4.815510
299.604126	8000.439859	10.011725	-0.060926	4.815493
299.364510	8000.373883	10.016730	-0.060882	4.815475
299.391181	8000.403189	10.021735	-0.060887	4.815483
299.284420	8000.298798	10.026739	-0.060867	4.815453
299.245629	8000.557913	10.031744	-0.060860	4.815529
299.626212	8000.445577	10.036749	-0.060930	4.815494
299.394496	8000.555042	10.041754	-0.060887	4.815528
299.650463	8000.402155	10.046759	-0.060935	4.815482
299.772247	8000.270557	10.051763	-0.060958	4.815443
299.794951	8000.520005	10.056768	-0.060962	4.815515
299.695982	8000.232949	10.061773	-0.060943	4.815432
299.671408	8000.314853	10.066778	-0.060939	4.815456
299.715507	8000.312379	10.071783	-0.060947	4.815455
299.681787	8000.380234	10.076787	-0.060941	4.815475
299.712384	8000.507951	10.081792	-0.060947	4.815512
299.877411	8000.274450	10.086797	-0.060977	4.815443
299.802307	8000.294584	10.091802	-0.060963	4.815449
299.444215	8000.328193	10.096807	-0.060897	4.815461
299.551575	8000.372735	10.101811	-0.060917	4.815473
299.645729	8000.440575	10.106816	-0.060934	4.815493
299.627079	8000.154854	10.111821	-0.060931	4.815409
299.593715	8000.383059	10.116826	-0.060925	4.815476
299.668423	8000.430266	10.121831	-0.060939	4.815490
299.825591	8000.211601	10.126835	-0.060968	4.815425
299.531512	8000.458996	10.131840	-0.060913	4.815499
299.640853	8000.297261	10.136845	-0.060933	4.815451
299.713065	8000.496220	10.141850	-0.060947	4.815509
299.810209	8000.555559	10.146855	-0.060965	4.815526
299.926342	8000.339417	10.151859	-0.060987	4.815462
299.865740	8000.430344	10.156864	-0.060975	4.815489
299.935542	8000.105470	10.161869	-0.060988	4.815394
299.742833	8000.335306	10.166874	-0.060952	4.815462
299.880230	8000.308726	10.171879	-0.060978	4.815453
299.772601	8000.167976	10.176883	-0.060958	4.815413
299.727991	8000.375684	10.181888	-0.060950	4.815473
299.812511	8000.231710	10.186893	-0.060965	4.815431
299.847352	8000.374462	10.191898	-0.060972	4.815473
299.867474	8000.336314	10.196903	-0.060976	4.815461
299.887232	8000.312057	10.201907	-0.060979	4.815454
299.754440	8000.437061	10.206912	-0.060955	4.815491
299.820727	8000.232922	10.211917	-0.060967	4.815431
299.669840	8000.535074	10.216922	-0.060939	4.815520
299.636015	8000.543065	10.221927	-0.060933	4.815523
299.906675	8000.376525	10.226931	-0.060983	4.815473
299.904549	8000.542182	10.231936	-0.060983	4.815521
299.953236	8000.306748	10.236941	-0.060992	4.815452
299.955435	8000.239441	10.241946	-0.060992	4.815433
299.779739	8000.399009	10.246951	-0.060960	4.815480
299.764360	8000.234134	10.251955	-0.060957	4.815432
299.784138	8000.414050	10.256960	-0.060960	4.815484
299.771150	8000.381767	10.261965	-0.060958	4.815475
299.787881	8000.242012	10.266970	-0.060961	4.815434
299.754266	8000.437076	10.271975	-0.060955	4.815491
299.924128	8000.349035	10.276979	-0.060987	4.815465
299.838984	8000.378622	10.281984	-0.060971	4.815474
299.788187	8000.407712	10.286989	-0.060961	4.815483
299.825797	8000.432924	10.291994	-0.060968	4.815490
299.927069	8000.428193	10.296999	-0.060987	4.815488
299.771204	8000.445917	10.302003	-0.060958	4.815494
299.989811	8000.510480	10.307008	-0.060999	4.815512
299.943775	8000.541786	10.312013	-0.060990	4.815521
299.991339	8000.402541	10.317018	-0.060999	4.815480
299.835572	8000.422404	10.322023	-0.060970	4.815487
300.011452	8000.388981	10.327027	-0.061003	4.815476
299.853440	8000.526394	10.332032	-0.060974	4.815517
299.958139	8000.343201	10.337037	-0.060993	4.815463
300.078295	8000.414681	10.342042	-0.061016	4.815483
299.986803	8000.319093	10.347047	-0.060998	4.815456
299.863977	8000.268952	10.352051	-0.060976	4.815442
299.754997	8000.514077	10.357056	-0.060955	4.815514
300.015235	8000.413639	10.362061	-0.061004	4.815483
299.855612	8000.382128	10.367066	-0.060974	4.815475
299.823520	8000.306769	10.372071	-0.060968	4.815453
299.977227	8000.313598	10.377075	-0.060997	4.815454
299.866604	8000.406901	10.382080	-0.060976	4.815482
299.802660	8000.292530	10.387085	-0.060964	4.815449
299.953350	8000.479965	10.392090	-0.060992	4.815503
299.976151	8000.334964	10.397095	-0.060997	4.815460
299.938146	8000.354645	10.402099	-0.060990	4.815466
300.067793	8000.431627	10.407104	-0.061014	4.815488
300.188083	8000.217693	10.412109	-0.061036	4.815425
300.082172	8000.431869	10.417114	-0.061016	4.815488
300.065761	8000.412356	10.422119	-0.061013	4.815483
300.054229	8000.375821	10.427123	-0.061011	4.815472
299.913918	8000.380975	10.432128	-0.060985	4.815474
300.197493	8000.394237	10.437133	-0.061038	4.815477
300.214067	8000.217063	10.442138	-0.061041	4.815425
300.213867	8000.385959	10.447143	-0.061041	4.815474
300.131900	8000.308702	10.452147	-0.061026	4.815452
300.142201	8000.276806	10.457152	-0.061028	4.815443
300.103578	8000.181028	10.462157	-0.061020	4.815415
300.136724	8000.306649	10.467162	-0.061027	4.815451
299.909308	8000.213081	10.472167	-0.060984	4.815425
300.115524	8000.254989	10.477171	-0.061023	4.815436
300.105625	8000.433344	10.482176	-0.061021	4.815488
300.046542	8000.367157	10.487181	-0.061010	4.815469
300.081861	8000.238399	10.492186	-0.061016	4.815432
300.161121	8000.377614	10.497191	-0.061031	4.815472
300.185800	8000.010300	10.502195	-0.061036	4.815365
300.154890	8000.195788	10.507200	-0.061030	4.815419
300.371361	8000.189762	10.512205	-0.061070	4.815416
300.250113	8000.092613	10.517210	-0.061048	4.815388
299.978137	8000.320065	10.522215	-0.060997	4.815456
300.103237	8000.221660	10.527219	-0.061021	4.815427
300.176893	8000.262436	10.532224	-0.061034	4.815438
300.222523	8000.144539	10.537229	-0.061043	4.815404
300.080191	8000.322833	10.542234	-0.061016	4.815456
299.948977	8000.385864	10.547239	-0.060992	4.815475
300.060002	8000.274397	10.552243	-0.061013	4.815442
299.959263	8000.343278	10.557248	-0.060994	4.815463
300.255412	8000.207092	10.562253	-0.061049	4.815422
300.245363	8000.263582	10.567258	-0.061047	4.815438
299.906356	8000.375542	10.572263	-0.060984	4.815473
300.149417	8000.340027	10.577267	-0.061029	4.815461
300.247324	8000.166342	10.582272	-0.061048	4.815410
300.217556	8000.317643	10.587277	-0.061042	4.815454
300.104567	8000.128699	10.592282	-0.061021	4.815399
300.282540	8000.328346	10.597287	-0.061054	4.815457
300.278291	8000.089896	10.602291	-0.061053	4.815387
300.148211	8000.270531	10.607296	-0.061029	4.815441
300.101546	8000.144689	10.612301	-0.061020	4.815404
300.383842	8000.171824	10.617306	-0.061073	4.815411
300.176448	8000.196176	10.622311	-0.061034	4.815419
300.319178	8000.172892	10.627315	-0.061061	4.815411
300.284451	8000.326249	10.632320	-0.061055	4.815456
300.282597	8000.354013	10.637325	-0.061054	4.815464
300.327310	8000.378274	10.642330	-0.061063	4.815471
300.382951	8000.229542	10.647335	-0.061073	4.815428
300.476188	8000.230022	10.652339	-0.061090	4.815427
300.319443	8000.154731	10.657344	-0.061061	4.815406
300.159739	8000.244013	10.662349	-0.061032	4.815433
300.270869	8000.401930	10.667354	-0.061052	4.815478
300.204054	8000.276820	10.672359	-0.061040	4.815442
300.265185	8000.228664	10.677363	-0.061051	4.815428
300.314003	8000.307511	10.682368	-0.061060	4.815451
300.461333	8000.152819	10.687373	-0.061088	4.815405
300.102394	8000.323242	10.692378	-0.061021	4.815456
300.181863	8000.537290	10.697383	-0.061036	4.815518
300.255751	8000.175065	10.702387	-0.061049	4.815412
300.046902	8000.413187	10.707392	-0.061011	4.815483
300.164068	8000.163926	10.712397	-0.061032	4.815409
300.302442	8000.254948	10.717402	-0.061058	4.815435
300.214569	8000.435217	10.722407	-0.061042	4.815488
300.266920	8000.402949	10.727411	-0.061052	4.815479
300.482489	8000.422565	10.732416	-0.061092	4.815483
300.462316	8000.265091	10.737421	-0.061088	4.815438
300.201795	8000.228698	10.742426	-0.061040	4.815428
300.316828	8000.424094	10.747431	-0.061061	4.815485
300.411962	8000.413916	10.752435	-0.061079	4.815481
300.257149	8000.333311	10.757440	-0.061050	4.815459
300.267989	8000.289664	10.762445	-0.061052	4.815446
300.539241	8000.186203	10.767450	-0.061102	4.815414
300.338494	8000.437288	10.772455	-0.061065	4.815488
300.341138	8000.399919	10.777459	-0.061066	4.815478
300.345179	8000.480161	10.782464	-0.061067	4.815501
300.431073	8000.138446	10.787469	-0.061082	4.815401
300.407247	8000.268467	10.792474	-0.061078	4.815439
300.429600	8000.468740	10.797479	-0.061082	4.815497
300.544748	8000.182027	10.802483	-0.061104	4.815413
300.260665	8000.410349	10.807488	-0.061051	4.815481
300.277883	8000.258842	10.812493	-0.061054	4.815437
300.428453	8000.428104	10.817498	-0.061082	4.815485
300.245643	8000.382310	10.822503	-0.061048	4.815473
300.316351	8000.165415	10.827507	-0.061061	4.815409
300.404356	8000.410604	10.832512	-0.061078	4.815480
300.600872	8000.402110	10.837517	-0.061114	4.815477
300.446904	8000.252035	10.842522	-0.061086	4.815434
300.425624	8000.381030	10.847527	-0.061082	4.815472
300.552015	8000.347853	10.852531	-0.061105	4.815461
300.180225	8000.350233	10.857536	-0.061036	4.815464
300.352909	8000.406551	10.862541	-0.061068	4.815479
300.481792	8000.125413	10.867546	-0.061092	4.815397
300.305797	8000.258252	10.872551	-0.061059	4.815436
300.491827	8000.176893	10.877555	-0.061094	4.815412
300.503292	8000.231602	10.882560	-0.061096	4.815428
300.472697	8000.252475	10.887565	-0.061090	4.815434
300.390397	8000.345180	10.892570	-0.061075	4.815461
300.332523	8000.382704	10.897575	-0.061064	4.815473
300.554768	8000.261325	10.902579	-0.061106	4.815436
300.396100	8000.451109	10.907584	-0.061076	4.815492
300.404691	8000.473701	10.912589	-0.061078	4.815499
300.675621	8000.267611	10.917594	-0.061128	4.815437
300.531096	8000.428768	10.922599	-0.061102	4.815485
300.437291	8000.335278	10.927603	-0.061084	4.815458
300.298900	8000.241050	10.932608	-0.061058	4.815431
300.417420	8000.420470	10.937613	-0.061080	4.815483
300.526207	8000.401967	10.942618	-0.061101	4.815477
300.615387	8000.311516	10.947623	-0.061117	4.815450
300.562917	8000.152438	10.952627	-0.061107	4.815404
300.312332	8000.323591	10.957632	-0.061061	4.815455
300.326496	8000.213723	10.962637	-0.061063	4.815423
300.480184	8000.210931	10.967642	-0.061092	4.815422
300.365699	8000.479484	10.972647	-0.061071	4.815501
300.519518	8000.207310	10.977651	-0.061099	4.815420
300.493151	8000.397153	10.982656	-0.061095	4.815476
300.597952	8000.274892	10.987661	-0.061114	4.815440
300.552414	8000.351104	10.992666	-0.061106	4.815462
300.391178	8000.421119	10.997671	-0.061076	4.815483
300.699753	8000.200689	11.002675	-0.061133	4.815418
300.588887	8000.318575	11.007680	-0.061112	4.815453
300.454238	8000.120718	11.012685	-0.061087	4.815395
300.464487	8000.238477	11.017690	-0.061089	4.815430
300.475099	8000.424657	11.022695	-0.061091	4.815484
300.471801	8000.243946	11.027699	-0.061091	4.815431
300.268729	8000.373129	11.032704	-0.061053	4.815470
300.339916	8000.146620	11.037709	-0.061066	4.815404
300.505220	8000.268022	11.042714	-0.061097	4.815438
300.655840	8000.206385	11.047719	-0.061125	4.815419
300.548491	8000.209949	11.052723	-0.061105	4.815421
300.489903	8000.361842	11.057728	-0.061094	4.815466
300.612877	8000.189641	11.062733	-0.061117	4.815415
300.700500	8000.356790	11.067738	-0.061133	4.815463
300.718432	8000.263018	11.072743	-0.061137	4.815436
300.772146	8000.357983	11.077747	-0.061147	4.815463
300.664730	8000.418202	11.082752	-0.061127	4.815481
300.713526	8000.234078	11.087757	-0.061136	4.815427
300.564963	8000.104405	11.092762	-0.061108	4.815390
300.381962	8000.330129	11.097767	-0.061074	4.815457
300.739352	7999.980095	11.102771	-0.061141	4.815353
300.685902	8000.295626	11.107776	-0.061131	4.815445
300.551608	8000.078533	11.112781	-0.061106	4.815383
300.655055	8000.253426	11.117786	-0.061125	4.815433
300.686912	8000.193024	11.122791	-0.061131	4.815415
300.592225	8000.202143	11.127795	-0.061113	4.815419
300.384142	8000.228621	11.132800	-0.061075	4.815427
300.677384	8000.234560	11.137805	-0.061129	4.815428
300.665284	8000.300638	11.142810	-0.061127	4.815447
300.593964	8000.235316	11.147815	-0.061114	4.815428
300.873524	8000.295547	11.152819	-0.061166	4.815444
300.754155	8000.230496	11.157824	-0.061144	4.815426
300.759613	8000.107655	11.162829	-0.061145	4.815390
300.768916	8000.061845	11.167834	-0.061146	4.815377
300.787948	8000.125231	11.172839	-0.061150	4.815395
300.632308	8000.131201	11.177843	-0.061121	4.815398
300.508325	8000.209317	11.182848	-0.061098	4.815421
300.688502	8000.131067	11.187853	-0.061131	4.815397
300.716647	8000.180709	11.192858	-0.061137	4.815412
300.545794	8000.431223	11.197863	-0.061105	4.815486
300.932731	8000.194989	11.202867	-0.061177	4.815415
300.768464	8000.300230	11.207872	-0.061147	4.815446
300.683031	8000.127776	11.212877	-0.061131	4.815396
300.661923	8000.080392	11.217882	-0.061127	4.815383
300.575244	8000.271370	11.222887	-0.061111	4.815439
300.841110	8000.224475	11.227891	-0.061160	4.815424
300.721798	8000.248151	11.232896	-0.061138	4.815431
300.776896	8000.172100	11.237901	-0.061148	4.815409
300.804472	8000.159732	11.242906	-0.061153	4.815405
300.829021	8000.286281	11.247911	-0.061158	4.815442
300.789459	8000.092139	11.252915	-0.061150	4.815385
300.702503	8000.227526	11.257920	-0.061134	4.815425
300.801384	8000.359586	11.262925	-0.061153	4.815464
300.742802	8000.187577	11.267930	-0.061142	4.815414
300.796913	8000.408688	11.272935	-0.061152	4.815478
300.760224	8000.179317	11.277939	-0.061145	4.815411
300.708223	8000.320630	11.282944	-0.061136	4.815453
300.740384	8000.375684	11.287949	-0.061142	4.815468
300.760898	8000.202850	11.292954	-0.061145	4.815418
300.605745	8000.414072	11.297959	-0.061117	4.815480
300.675427	8000.190743	11.302963	-0.061129	4.815415
300.975218	8000.383865	11.307968	-0.061185	4.815470
300.759183	8000.332174	11.312973	-0.061145	4.815456
300.777388	8000.152888	11.317978	-0.061148	4.815403
300.904827	8000.396597	11.322983	-0.061172	4.815474
301.008614	8000.204834	11.327987	-0.061192	4.815417
300.822986	8000.238099	11.332992	-0.061157	4.815428
300.868866	8000.273070	11.337997	-0.061166	4.815438
301.014325	8000.226313	11.343002	-0.061193	4.815424
300.721447	8000.414938	11.348007	-0.061138	4.815480
300.874476	8000.106405	11.353011	-0.061167	4.815389
300.936288	8000.230366	11.358016	-0.061178	4.815425
300.938334	8000.319127	11.363021	-0.061179	4.815451
300.939605	8000.105352	11.368026	-0.061179	4.815389
300.705101	8000.285325	11.373031	-0.061135	4.815442
300.701320	8000.182641	11.378035	-0.061134	4.815412
300.765875	8000.241440	11.383040	-0.061147	4.815429
300.745317	8000.081822	11.388045	-0.061143	4.815383
300.804678	8000.262397	11.393050	-0.061154	4.815435
300.742680	8000.183333	11.398055	-0.061142	4.815412
300.856631	8000.403301	11.403059	-0.061164	4.815476
300.717094	8000.306913	11.408064	-0.061138	4.815449
300.646339	8000.259773	11.413069	-0.061124	4.815435
300.681359	8000.216528	11.418074	-0.061131	4.815422
300.735930	8000.261264	11.423079	-0.061141	4.815435
300.870494	8000.213257	11.428083	-0.061166	4.815420
300.638221	8000.242540	11.433088	-0.061123	4.815430
300.670427	8000.524221	11.438093	-0.061129	4.815512
300.799063	8000.366009	11.443098	-0.061153	4.815465
300.797306	8000.358499	11.448103	-0.061153	4.815463
300.693266	8000.270184	11.453107	-0.061133	4.815438
300.681031	8000.292431	11.458112	-0.061131	4.815444
300.596156	8000.170228	11.463117	-0.061115	4.815409
300.717124	8000.092065	11.468122	-0.061138	4.815386
300.746864	8000.284976	11.473127	-0.061143	4.815442
301.032509	8000.223444	11.478131	-0.061196	4.815423
300.655266	8000.361494	11.483136	-0.061126	4.815465
300.562124	8000.280844	11.488141	-0.061109	4.815442
300.756978	8000.125871	11.493146	-0.061145	4.815395
300.820527	8000.217791	11.498151	-0.061157	4.815422
300.623050	8000.065926	11.503155	-0.061120	4.815379
300.742940	8000.288127	11.508160	-0.061143	4.815443
300.801818	8000.217484	11.513165	-0.061154	4.815422
300.734371	7999.996157	11.518170	-0.061141	4.815358
300.576355	8000.314228	11.523175	-0.061112	4.815451
301.078187	8000.021108	11.528179	-0.061205	4.815363
301.033352	8000.248059	11.533184	-0.061197	4.815430
300.916880	8000.178780	11.538189	-0.061175	4.815410
300.951858	8000.132327	11.543194	-0.061182	4.815396
300.735408	8000.371394	11.548199	-0.061141	4.815467
300.894911	8000.076866	11.553203	-0.061171	4.815380
300.807147	8000.121376	11.558208	-0.061155	4.815394
300.794022	8000.285783	11.563213	-0.061152	4.815442
300.945644	8000.139713	11.568218	-0.061180	4.815399
300.796081	8000.160749	11.573223	-0.061153	4.815405
300.910878	8000.034379	11.578227	-0.061174	4.815368
301.049858	8000.131827	11.583232	-0.061200	4.815396
300.998036	8000.266729	11.588237	-0.061190	4.815435
301.226366	8000.158278	11.593242	-0.061233	4.815403
301.066205	8000.175930	11.598247	-0.061203	4.815409
301.103658	8000.096380	11.603251	-0.061210	4.815385
300.959978	8000.083306	11.608256	-0.061183	4.815382
300.874310	8000.187714	11.613261	-0.061167	4.815413
300.861655	8000.127642	11.618266	-0.061165	4.815395
300.755826	8000.288372	11.623271	-0.061145	4.815443
300.979995	7999.991711	11.628275	-0.061187	4.815355
300.913319	8000.148815	11.633280	-0.061175	4.815401
300.826520	8000.164478	11.638285	-0.061159	4.815406
300.870833	8000.183388	11.643290	-0.061167	4.815412
300.977434	8000.205470	11.648295	-0.061187	4.815418
300.973391	8000.095299	11.653299	-0.061186	4.815385
300.890870	8000.228622	11.658304	-0.061171	4.815425
300.859529	8000.147929	11.663309	-0.061165	4.815401
301.068740	8000.157818	11.668314	-0.061204	4.815403
301.037231	8000.222505	11.673319	-0.061198	4.815422
300.919022	8000.080506	11.678323	-0.061176	4.815381
300.950760	8000.039344	11.683328	-0.061182	4.815369
300.866746	8000.142711	11.688333	-0.061166	4.815400
301.028858	7999.978643	11.693338	-0.061196	4.815351
300.768561	8000.087635	11.698343	-0.061148	4.815384
300.855605	7999.964011	11.703347	-0.061164	4.815348
300.988852	8000.007914	11.708352	-0.061189	4.815360
301.010231	7999.939856	11.713357	-0.061193	4.815340
301.019533	8000.006288	11.718362	-0.061195	4.815359
300.744432	8000.183449	11.723367	-0.061143	4.815412
300.937628	8000.090449	11.728371	-0.061179	4.815384
300.944756	8000.156846	11.733376	-0.061181	4.815404
300.903046	8000.336814	11.738381	-0.061173	4.815456
301.018348	8000.043689	11.743386	-0.061194	4.815370
301.164555	8000.247088	11.748391	-0.061222	4.815429
301.183580	8000.050711	11.753395	-0.061225	4.815371
300.965101	8000.270503	11.758400	-0.061185	4.815437
300.919491	8000.179952	11.763405	-0.061176	4.815410
300.871303	7999.965358	11.768410	-0.061167	4.815348
300.832837	8000.213792	11.773415	-0.061160	4.815421
300.810003	8000.172793	11.778419	-0.061156	4.815409
301.004835	8000.106545	11.783424	-0.061192	4.815389
300.860407	8000.135149	11.788429	-0.061165	4.815398
300.915184	8000.136060	11.793434	-0.061175	4.815398
300.808367	8000.197358	11.798439	-0.061156	4.815416
300.813837	8000.033896	11.803443	-0.061157	4.815368
300.957394	8000.170972	11.808448	-0.061183	4.815408
301.138117	8000.206044	11.813453	-0.061217	4.815417
301.324529	8000.150347	11.818458	-0.061252	4.815400
300.822675	8000.269224	11.823463	-0.061158	4.815437
301.012926	8000.246729	11.828467	-0.061194	4.815429
301.122993	8000.124555	11.833472	-0.061214	4.815393
300.902893	8000.133730	11.838477	-0.061173	4.815397
301.007118	8000.235947	11.843482	-0.061193	4.815426
301.005350	8000.239126	11.848487	-0.061192	4.815427
301.154312	8000.164633	11.853491	-0.061220	4.815405
301.162701	8000.132704	11.858496	-0.061222	4.815395
300.986788	8000.122302	11.863501	-0.061189	4.815393
301.078113	8000.212545	11.868506	-0.061206	4.815419
300.916372	8000.284690	11.873511	-0.061176	4.815441
301.171094	8000.128573	11.878515	-0.061223	4.815394
301.116506	8000.155462	11.883520	-0.061213	4.815402
301.055739	8000.323355	11.888525	-0.061202	4.815452
301.183683	8000.205753	11.893530	-0.061226	4.815417
301.163698	8000.301632	11.898535	-0.061222	4.815445
301.136436	8000.051037	11.903539	-0.061217	4.815372
301.072144	7999.998660	11.908544	-0.061205	4.815357
301.002131	8000.226262	11.913549	-0.061192	4.815424
301.040646	8000.262179	11.918554	-0.061199	4.815434
300.924784	8000.407778	11.923559	-0.061178	4.815477
300.907257	8000.078239	11.928563	-0.061174	4.815381
301.082022	8000.093970	11.933568	-0.061207	4.815385
300.974210	8000.207632	11.938573	-0.061187	4.815418
300.967962	8000.135907	11.943578	-0.061186	4.815397
300.891841	8000.229784	11.948583	-0.061172	4.815425
301.055348	8000.056118	11.953587	-0.061202	4.815374
300.899080	8000.047111	11.958592	-0.061173	4.815372
300.816454	8000.247778	11.963597	-0.061158	4.815431
301.107488	8000.195956	11.968602	-0.061212	4.815414
301.033851	8000.305910	11.973607	-0.061198	4.815447
300.981950	8000.208840	11.978611	-0.061188	4.815419
301.289091	8000.091008	11.983616	-0.061246	4.815383
301.307394	8000.100934	11.988621	-0.061249	4.815385
301.144329	7999.945363	11.993626	-0.061219	4.815341
301.021858	8000.220198	11.998631	-0.061196	4.815422
301.207618	7999.961382	12.003635	-0.061230	4.815345
301.149321	8000.179557	12.008640	-0.061220	4.815409
301.044398	8000.201334	12.013645	-0.061200	4.815416
301.311728	8000.020840	12.018650	-0.061250	4.815362
301.324720	8000.125817	12.023655	-0.061252	4.815393
301.154133	8000.135814	12.028659	-0.061221	4.815396
301.091892	7999.999021	12.033664	-0.061209	4.815357
301.233548	8000.095445	12.038669	-0.061235	4.815384
301.250069	8000.120307	12.043674	-0.061239	4.815391
301.279936	8000.052389	12.048679	-0.061244	4.815371
301.266410	8000.084236	12.053683	-0.061242	4.815381
301.166460	8000.152062	12.058688	-0.061223	4.815401
301.100477	8000.238624	12.063693	-0.061211	4.815427
301.337366	8000.080073	12.068698	-0.061255	4.815379
301.264889	8000.143010	12.073703	-0.061241	4.815398
301.098583	8000.224700	12.078707	-0.061211	4.815423
301.222613	8000.229968	12.083712	-0.061234	4.815424
301.184151	8000.185502	12.088717	-0.061226	4.815411
301.406448	8000.131469	12.093722	-0.061268	4.815394
301.253861	8000.170627	12.098727	-0.061239	4.815406
301.349901	8000.141223	12.103731	-0.061257	4.815397
301.115218	8000.282710	12.108736	-0.061214	4.815439
301.091931	8000.079217	12.113741	-0.061209	4.815380
301.306325	8000.180056	12.118746	-0.061249	4.815409
301.226259	8000.203314	12.123751	-0.061234	4.815416
301.175937	7999.969441	12.128755	-0.061225	4.815348
301.312327	8000.005914	12.133760	-0.061250	4.815358
301.368511	8000.173611	12.138765	-0.061261	4.815406
301.258984	7999.946237	12.143770	-0.061240	4.815340
301.257389	8000.117250	12.148775	-0.061240	4.815390
301.231801	8000.092239	12.153779	-0.061235	4.815383
301.289815	8000.163757	12.158784	-0.061246	4.815404
301.197421	8000.228502	12.163789	-0.061229	4.815423
301.339174	8000.139993	12.168794	-0.061256	4.815397
301.349150	8000.126263	12.173799	-0.061257	4.815393
301.176815	7999.999400	12.178803	-0.061225	4.815356
301.254349	8000.219832	12.183808	-0.061240	4.815420
301.116852	8000.079650	12.188813	-0.061214	4.815380
301.182724	7999.986675	12.193818	-0.061226	4.815353
301.036463	8000.209803	12.198823	-0.061199	4.815419
301.103155	8000.017426	12.203827	-0.061212	4.815362
301.032276	8000.162701	12.208832	-0.061199	4.815405
301.022698	8000.099473	12.213837	-0.061197	4.815386
301.286225	8000.129506	12.218842	-0.061246	4.815394
301.175853	8000.121261	12.223847	-0.061225	4.815392
301.181005	8000.018725	12.228851	-0.061226	4.815362
301.257121	8000.075577	12.233856	-0.061240	4.815378
301.217551	8000.167924	12.238861	-0.061233	4.815405
301.303284	8000.149038	12.243866	-0.061249	4.815399
301.081677	8000.140014	12.248871	-0.061208	4.815398
301.102259	8000.157461	12.253875	-0.061212	4.815403
301.170691	8000.089115	12.258880	-0.061224	4.815383
301.105767	8000.090176	12.263885	-0.061212	4.815383
301.241008	8000.140527	12.268890	-0.061238	4.815397
301.330020	8000.143076	12.273895	-0.061254	4.815398
301.178672	8000.067873	12.278899	-0.061226	4.815376
301.276265	7999.983976	12.283904	-0.061244	4.815351
301.203684	8000.338746	12.288909	-0.061231	4.815455
301.266226	7999.954949	12.293914	-0.061242	4.815343
301.100960	8000.091174	12.298919	-0.061212	4.815384
301.211015	8000.144314	12.303923	-0.061232	4.815399
301.263715	8000.035085	12.308928	-0.061242	4.815366
301.066717	8000.322581	12.313933	-0.061205	4.815451
301.266085	8000.030851	12.318938	-0.061242	4.815365
301.415114	8000.318749	12.323943	-0.061270	4.815449
301.300958	8000.119090	12.328947	-0.061249	4.815391
301.341116	8000.082343	12.333952	-0.061256	4.815380
301.322571	8000.095934	12.338957	-0.061253	4.815384
301.367071	8000.083846	12.343962	-0.061261	4.815380
301.140628	8000.363371	12.348967	-0.061219	4.815463
301.173725	8000.173640	12.353971	-0.061225	4.815407
301.233217	8000.249459	12.358976	-0.061236	4.815429
301.293823	8000.201293	12.363981	-0.061248	4.815415
301.439357	8000.043362	12.368986	-0.061275	4.815368
301.456054	8000.227508	12.373991	-0.061278	4.815422
301.526129	7999.936838	12.378995	-0.061291	4.815336
301.548130	8000.155279	12.384000	-0.061295	4.815400
301.278252	8000.142247	12.389005	-0.061245	4.815398
301.505014	7999.950388	12.394010	-0.061287	4.815340
301.146787	8000.059892	12.399015	-0.061220	4.815374
301.224773	8000.083637	12.404019	-0.061235	4.815381
301.291522	8000.024883	12.409024	-0.061247	4.815363
301.211321	8000.228799	12.414029	-0.061233	4.815423
301.267178	7999.973171	12.419034	-0.061243	4.815348
301.243847	8000.096787	12.424039	-0.061239	4.815385
301.471635	8000.016120	12.429043	-0.061281	4.815360
301.244305	8000.167351	12.434048	-0.061239	4.815405
301.270276	8000.179542	12.439053	-0.061244	4.815409
301.325711	8000.082117	12.444058	-0.061254	4.815380
301.378695	8000.250830	12.449063	-0.061264	4.815429
301.310548	8000.012383	12.454067	-0.061251	4.815360
301.213454	8000.185018	12.459072	-0.061233	4.815410
301.215167	8000.368915	12.464077	-0.061233	4.815464
301.107814	8000.051781	12.469082	-0.061213	4.815372
301.174915	8000.281660	12.474087	-0.061226	4.815439
301.368201	8000.140557	12.479091	-0.061262	4.815397
301.264090	8000.057586	12.484096	-0.061242	4.815373
301.277572	8000.164711	12.489101	-0.061245	4.815404
301.518035	8000.047909	12.494106	-0.061290	4.815369
301.356579	8000.106162	12.499111	-0.061260	4.815387
301.341971	7999.930607	12.504115	-0.061257	4.815335
301.308906	8000.020923	12.509120	-0.061251	4.815362
301.205121	8000.129306	12.514125	-0.061232	4.815394
301.345100	7999.941353	12.519130	-0.061258	4.815339
301.243979	7999.932192	12.524135	-0.061239	4.815336
301.369962	8000.090357	12.529139	-0.061262	4.815382
301.516094	8000.090647	12.534144	-0.061290	4.815381
301.111468	8000.140586	12.539149	-0.061214	4.815398
301.378671	8000.063781	12.544154	-0.061264	4.815374
301.220272	8000.011979	12.549159	-0.061234	4.815360
301.061301	8000.176102	12.554163	-0.061205	4.815409
301.281421	8000.168000	12.559168	-0.061246	4.815405
301.403014	8000.360303	12.564173	-0.061269	4.815461
301.529049	8000.249083	12.569178	-0.061292	4.815428
301.432966	8000.342630	12.574183	-0.061274	4.815455
301.598782	8000.190380	12.579187	-0.061305	4.815410
301.478819	8000.310255	12.584192	-0.061283	4.815446
301.281350	8000.358289	12.589197	-0.061246	4.815461
301.518396	8000.102460	12.594202	-0.061290	4.815385
301.366651	8000.073217	12.599207	-0.061262	4.815377
301.342699	8000.202168	12.604211	-0.061258	4.815415
301.495365	8000.169428	12.609216	-0.061286	4.815404
301.480458	8000.229046	12.614221	-0.061283	4.815422
301.499981	8000.219751	12.619226	-0.061287	4.815419
301.517288	8000.192245	12.624231	-0.061290	4.815411
301.477007	8000.158439	12.629235	-0.061283	4.815401
301.356261	8000.367028	12.634240	-0.061260	4.815463
301.213263	8000.279134	12.639245	-0.061234	4.815438
301.430204	7999.869039	12.644250	-0.061274	4.815317
301.289395	8000.068740	12.649255	-0.061248	4.815376
301.308862	8000.112893	12.654259	-0.061251	4.815389
301.534438	8000.080295	12.659264	-0.061293	4.815378
301.553344	8000.397035	12.664269	-0.061297	4.815471
301.653687	8000.013862	12.669274	-0.061315	4.815358
301.392009	8000.068313	12.674279	-0.061267	4.815375
301.335026	8000.135783	12.679283	-0.061256	4.815395
301.391835	8000.154901	12.684288	-0.061267	4.815401
301.227250	8000.148962	12.689293	-0.061236	4.815400
301.342635	8000.296263	12.694298	-0.061258	4.815442
301.168383	8000.088124	12.699303	-0.061225	4.815382
301.216925	8000.343352	12.704307	-0.061234	4.815457
301.339674	8000.063177	12.709312	-0.061257	4.815374
301.338625	8000.190371	12.714317	-0.061257	4.815411
301.399415	7999.902755	12.719322	-0.061268	4.815327
301.260814	8000.055458	12.724327	-0.061243	4.815372
301.313319	8000.054193	12.729331	-0.061252	4.815372
301.582206	8000.027658	12.734336	-0.061302	4.815363
301.470644	8000.262055	12.739341	-0.061282	4.815432
301.430527	7999.926796	12.744346	-0.061274	4.815334
301.436260	8000.174898	12.749351	-0.061275	4.815406
301.227327	8000.092324	12.754355	-0.061236	4.815383
301.311029	8000.047749	12.759360	-0.061252	4.815370
301.269487	8000.344241	12.764365	-0.061244	4.815457
301.291555	8000.191742	12.769370	-0.061248	4.815412
301.322219	8000.225391	12.774375	-0.061254	4.815422
301.489233	8000.112715	12.779379	-0.061285	4.815388
301.418130	8000.179951	12.784384	-0.061272	4.815408
301.201620	8000.174219	12.789389	-0.061232	4.815407
301.357164	8000.202459	12.794394	-0.061261	4.815415
301.313650	8000.411262	12.799399	-0.061253	4.815476
301.215583	8000.203317	12.804403	-0.061234	4.815416
301.498013	8000.042315	12.809408	-0.061287	4.815367
301.426034	8000.180090	12.814413	-0.061274	4.815408
301.339486	8000.221414	12.819418	-0.061258	4.815420
301.450263	8000.210427	12.824423	-0.061278	4.815417
301.473364	8000.316644	12.829427	-0.061283	4.815448
301.454123	8000.087559	12.834432	-0.061279	4.815381
301.287282	8000.179931	12.839437	-0.061248	4.815409
301.471568	8000.155198	12.844442	-0.061282	4.815400
301.475616	8000.076161	12.849447	-0.061283	4.815377
301.488054	8000.084921	12.854451	-0.061285	4.815380
301.489838	7999.926742	12.859456	-0.061285	4.815334
301.560991	8000.173793	12.864461	-0.061299	4.815405
301.610689	8000.068789	12.869466	-0.061308	4.815375
301.375257	8000.184608	12.874471	-0.061264	4.815409
301.399611	8000.217084	12.879475	-0.061269	4.815419
301.476658	8000.067636	12.884480	-0.061283	4.815375
301.379901	8000.181482	12.889485	-0.061265	4.815409
301.434210	8000.099004	12.894490	-0.061275	4.815384
301.456786	8000.235143	12.899495	-0.061280	4.815424
301.553552	8000.118092	12.904499	-0.061298	4.815389
301.486154	7999.995109	12.909504	-0.061285	4.815354
301.369566	8000.086177	12.914509	-0.061263	4.815381
301.593506	7999.914582	12.919514	-0.061305	4.815330
301.487382	8000.212139	12.924519	-0.061285	4.815417
301.482373	8000.265508	12.929523	-0.061285	4.815433
301.581979	8000.137814	12.934528	-0.061303	4.815395
301.512059	8000.076790	12.939533	-0.061290	4.815377
301.639445	8000.103494	12.944538	-0.061314	4.815385
301.480991	8000.374529	12.949543	-0.061284	4.815464
301.628077	8000.214484	12.954547	-0.061312	4.815417
301.345195	8000.122129	12.959552	-0.061259	4.815391
301.558152	8000.319157	12.964557	-0.061299	4.815448
301.612670	8000.154368	12.969562	-0.061309	4.815399
301.665586	8000.110350	12.974567	-0.061319	4.815386
301.669080	8000.062305	12.979571	-0.061319	4.815372
301.607138	8000.131831	12.984576	-0.061308	4.815393
301.642578	8000.283151	12.989581	-0.061315	4.815437
301.558896	8000.119274	12.994586	-0.061299	4.815390
301.495813	8000.103261	12.999591	-0.061287	4.815385
301.705308	8000.076810	13.004595	-0.061326	4.815376
301.515791	8000.105734	13.009600	-0.061291	4.815386
301.386000	8000.293861	13.014605	-0.061267	4.815441
301.537330	8000.081507	13.019610	-0.061295	4.815379
301.465707	8000.185081	13.024615	-0.061282	4.815409
301.416384	8000.234506	13.029619	-0.061273	4.815424
301.554889	8000.063630	13.034624	-0.061298	4.815373
301.544900	8000.245195	13.039629	-0.061296	4.815426
301.647593	7999.991412	13.044634	-0.061315	4.815352
301.742589	8000.230309	13.049639	-0.061333	4.815421
301.480635	8000.109438	13.054643	-0.061284	4.815387
301.439875	8000.219938	13.059648	-0.061277	4.815419
301.389617	8000.371972	13.064653	-0.061268	4.815464
301.682261	8000.167309	13.069658	-0.061322	4.815403
301.411601	8000.205575	13.074663	-0.061272	4.815415
301.331172	8000.220276	13.079667	-0.061257	4.815420
301.703341	8000.026556	13.084672	-0.061326	4.815362
301.528671	8000.387117	13.089677	-0.061294	4.815468
301.707818	8000.086496	13.094682	-0.061327	4.815379
301.671849	8000.130798	13.099687	-0.061320	4.815392
301.508907	8000.044712	13.104691	-0.061290	4.815368
301.448328	8000.054397	13.109696	-0.061279	4.815371
301.477248	8000.069845	13.114701	-0.061284	4.815375
301.455548	7999.966863	13.119706	-0.061280	4.815345
301.579349	8000.119648	13.124711	-0.061303	4.815390
301.510136	8000.208296	13.129715	-0.061290	4.815416
301.505221	8000.130178	13.134720	-0.061289	4.815393
301.509756	8000.316261	13.139725	-0.061290	4.815447
301.485185	8000.165125	13.144730	-0.061286	4.815403
301.409876	8000.154255	13.149735	-0.061272	4.815400
301.563665	8000.429407	13.154739	-0.061300	4.815480
301.457316	8000.125113	13.159744	-0.061280	4.815392
301.421556	8000.251732	13.164749	-0.061274	4.815429
301.442097	8000.310870	13.169754	-0.061278	4.815446
301.395783	8000.294066	13.174759	-0.061269	4.815441
301.389353	8000.192406	13.179763	-0.061268	4.815412
301.441644	8000.199690	13.184768	-0.061278	4.815414
301.385611	8000.272521	13.189773	-0.061267	4.815435
301.488107	8000.090357	13.194778	-0.061286	4.815381
301.487713	8000.329808	13.199783	-0.061286	4.815451
301.400738	8000.208637	13.204787	-0.061270	4.815416
301.574070	8000.192275	13.209792	-0.061302	4.815411
301.417936	8000.167234	13.214797	-0.061273	4.815404
301.531310	8000.245017	13.219802	-0.061294	4.815426
301.652469	8000.232065	13.224807	-0.061317	4.815422
301.524194	8000.376390	13.229811	-0.061293	4.815465
301.666026	8000.153187	13.234816	-0.061320	4.815399
301.546429	8000.437696	13.239821	-0.061297	4.815483
301.532891	8000.210842	13.244826	-0.061295	4.815416
301.446182	8000.178402	13.249831	-0.061279	4.815407
301.446649	8000.239344	13.254835	-0.061279	4.815425
301.535589	8000.262203	13.259840	-0.061295	4.815431
301.509855	8000.316296	13.264845	-0.061291	4.815447
301.615925	8000.333026	13.269850	-0.061310	4.815452
301.502671	8000.249901	13.274855	-0.061289	4.815428
301.345126	8000.425810	13.279859	-0.061260	4.815480
301.750838	8000.229439	13.284864	-0.061336	4.815421
301.778550	8000.320767	13.289869	-0.061341	4.815447
301.768762	8000.220118	13.294874	-0.061339	4.815418
301.557064	8000.291434	13.299879	-0.061300	4.815440
301.462081	8000.392482	13.304883	-0.061282	4.815470
301.618317	8000.163104	13.309888	-0.061311	4.815402
301.378223	8000.421024	13.314893	-0.061266	4.815478
301.425319	8000.190902	13.319898	-0.061275	4.815411
301.522186	8000.404176	13.324903	-0.061293	4.815473
301.575234	8000.420025	13.329907	-0.061303	4.815477
301.859718	8000.233399	13.334912	-0.061356	4.815421
301.791430	8000.484554	13.339917	-0.061343	4.815495
301.771732	8000.153902	13.344922	-0.061340	4.815399
301.641432	8000.188086	13.349927	-0.061315	4.815409
301.650315	8000.164716	13.354931	-0.061317	4.815402
301.589604	8000.256713	13.359936	-0.061306	4.815429
301.654478	8000.351865	13.364941	-0.061318	4.815457
301.847637	8000.224655	13.369946	-0.061354	4.815419
301.808662	8000.154524	13.374951	-0.061347	4.815399
301.601283	8000.241946	13.379955	-0.061308	4.815425
301.673821	8000.183288	13.384960	-0.061321	4.815408
301.728504	8000.375551	13.389965	-0.061332	4.815464
301.913014	8000.151986	13.394970	-0.061366	4.815397
301.617767	8000.126773	13.399975	-0.061311	4.815391
301.679463	8000.336255	13.404979	-0.061323	4.815452
301.739632	8000.053969	13.409984	-0.061334	4.815370
301.540352	8000.312567	13.414989	-0.061297	4.815446
301.597512	8000.171340	13.419994	-0.061307	4.815404
301.640204	8000.046977	13.424999	-0.061315	4.815368
301.467974	8000.331679	13.430003	-0.061283	4.815452
301.628581	8000.095961	13.435008	-0.061313	4.815382
301.784208	8000.302727	13.440013	-0.061342	4.815442
301.769383	8000.263998	13.445018	-0.061340	4.815431
301.725360	8000.423620	13.450023	-0.061331	4.815478
301.557587	8000.542702	13.455027	-0.061300	4.815513
301.649285	8000.234213	13.460032	-0.061317	4.815423
301.501983	8000.290562	13.465037	-0.061290	4.815440
301.704045	8000.119672	13.470042	-0.061327	4.815389
301.833352	8000.301415	13.475047	-0.061352	4.815441
301.658509	8000.209784	13.480051	-0.061319	4.815415
301.797044	8000.135118	13.485056	-0.061345	4.815393
301.843018	8000.263095	13.490061	-0.061353	4.815430
301.858735	8000.233425	13.495066	-0.061356	4.815421
301.527861	8000.192653	13.500071	-0.061295	4.815411
301.522216	8000.225700	13.505075	-0.061294	4.815421
301.733016	8000.177890	13.510080	-0.061333	4.815406
301.512285	8000.262953	13.515085	-0.061292	4.815432
301.556713	8000.181379	13.520090	-0.061300	4.815408
301.769767	8000.185988	13.525095	-0.061340	4.815408
301.674469	8000.369345	13.530099	-0.061322	4.815462
301.623159	8000.095897	13.535104	-0.061312	4.815382
301.698747	8000.206192	13.540109	-0.061327	4.815414
301.749025	8000.294687	13.545114	-0.061336	4.815440
301.633043	8000.347282	13.550119	-0.061314	4.815456
301.467351	8000.433258	13.555123	-0.061284	4.815482
301.752614	8000.293682	13.560128	-0.061337	4.815439
301.500136	8000.362182	13.565133	-0.061290	4.815461
301.526915	8000.188380	13.570138	-0.061295	4.815410
301.652647	8000.253541	13.575143	-0.061318	4.815428
301.666886	8000.204605	13.580147	-0.061321	4.815414
301.593069	8000.223691	13.585152	-0.061307	4.815420
301.584314	8000.239582	13.590157	-0.061305	4.815424
301.765169	8000.274658	13.595162	-0.061339	4.815434
301.660863	8000.179923	13.600167	-0.061320	4.815407
301.499916	8000.249943	13.605171	-0.061290	4.815428
301.728388	8000.108355	13.610176	-0.061332	4.815385
301.580117	8000.217070	13.615181	-0.061305	4.815418
301.553290	8000.029551	13.620186	-0.061300	4.815363
301.624765	8000.334336	13.625191	-0.061313	4.815452
301.819293	8000.197528	13.630195	-0.061349	4.815411
301.864234	7999.976993	13.635200	-0.061358	4.815346
301.782279	8000.165915	13.640205	-0.061342	4.815402
301.813328	8000.186743	13.645210	-0.061348	4.815408
301.732899	8000.104164	13.650215	-0.061333	4.815384
301.629686	8000.258526	13.655219	-0.061314	4.815430
301.922831	8000.120149	13.660224	-0.061369	4.815388
301.736735	8000.137371	13.665229	-0.061334	4.815394
301.549767	8000.089369	13.670234	-0.061299	4.815381
301.607672	8000.027261	13.675239	-0.061310	4.815362
301.798784	7999.968435	13.680243	-0.061345	4.815344
301.707449	8000.157201	13.685248	-0.061329	4.815400
301.537446	8000.165069	13.690253	-0.061297	4.815403
301.827297	8000.196609	13.695258	-0.061351	4.815411
301.797555	8000.168323	13.700263	-0.061345	4.815403
301.651791	8000.294184	13.705267	-0.061318	4.815440
301.770053	8000.143281	13.710272	-0.061340	4.815395
301.737437	8000.464514	13.715277	-0.061334	4.815489
301.585906	8000.419237	13.720282	-0.061306	4.815477
301.759627	8000.366535	13.725287	-0.061339	4.815461
301.561065	8000.397446	13.730291	-0.061302	4.815471
301.755874	8000.120603	13.735296	-0.061338	4.815389
301.593195	8000.371257	13.740301	-0.061308	4.815463
301.690694	8000.134489	13.745306	-0.061326	4.815393
301.648954	8000.135936	13.750311	-0.061318	4.815394
301.630911	8000.268194	13.755315	-0.061315	4.815433
301.840140	8000.205392	13.760320	-0.061354	4.815413
301.780118	8000.317712	13.765325	-0.061342	4.815446
301.580134	8000.036450	13.770330	-0.061305	4.815365
301.666238	8000.128746	13.775335	-0.061321	4.815392
301.616841	8000.289347	13.780339	-0.061312	4.815439
301.600152	7999.982268	13.785344	-0.061309	4.815349
301.518843	8000.390347	13.790349	-0.061294	4.815469
301.665611	8000.223882	13.795354	-0.061321	4.815419
301.855103	8000.343554	13.800359	-0.061357	4.815454
301.696110	8000.304568	13.805363	-0.061327	4.815443
301.703451	8000.048130	13.810368	-0.061328	4.815368
301.785378	8000.210911	13.815373	-0.061344	4.815415
301.833886	8000.146509	13.820378	-0.061353	4.815396
301.874722	8000.155740	13.825383	-0.061360	4.815399
301.755952	8000.376123	13.830387	-0.061338	4.815464
301.728507	8000.043207	13.835392	-0.061333	4.815366
301.748940	8000.163276	13.840397	-0.061337	4.815401
301.864167	8000.033704	13.845402	-0.061358	4.815363
301.992002	8000.119211	13.850407	-0.061382	4.815387
301.852387	8000.247312	13.855411	-0.061356	4.815425
301.847382	7999.932944	13.860416	-0.061355	4.815334
301.849967	8000.204514	13.865421	-0.061356	4.815413
301.633565	8000.115401	13.870426	-0.061315	4.815388
301.622872	8000.213573	13.875431	-0.061313	4.815417
301.848709	8000.195945	13.880435	-0.061356	4.815410
301.776618	7999.976673	13.885440	-0.061342	4.815347
301.675636	8000.085104	13.890445	-0.061323	4.815379
301.707763	8000.179711	13.895450	-0.061329	4.815406
301.779560	8000.040865	13.900455	-0.061343	4.815365
301.577955	8000.057830	13.905459	-0.061305	4.815371
301.744274	8000.136492	13.910464	-0.061336	4.815394
301.956306	8000.320679	13.915469	-0.061376	4.815446
301.737981	8000.384401	13.920474	-0.061335	4.815466
302.005542	8000.040349	13.925479	-0.061385	4.815364
301.830924	8000.168938	13.930483	-0.061352	4.815403
301.852745	8000.169302	13.935488	-0.061356	4.815403
301.887170	8000.198738	13.940493	-0.061363	4.815411
301.874983	8000.124775	13.945498	-0.061361	4.815390
301.854208	8000.064567	13.950503	-0.061357	4.815372
301.720109	8000.218416	13.955507	-0.061332	4.815418
301.788118	8000.203512	13.960512	-0.061344	4.815413
301.742767	8000.151448	13.965517	-0.061336	4.815398
301.747421	8000.183597	13.970522	-0.061337	4.815407
301.787699	8000.165025	13.975527	-0.061344	4.815402
301.825567	8000.236210	13.980531	-0.061352	4.815422
301.975535	8000.091179	13.985536	-0.061379	4.815379
301.784488	8000.310361	13.990541	-0.061344	4.815444
301.968811	8000.065414	13.995546	-0.061378	4.815372
301.862227	8000.142751	14.000551	-0.061358	4.815395
301.870099	8000.205955	14.005555	-0.061360	4.815413
301.763855	7999.916631	14.010560	-0.061340	4.815329
301.814234	8000.208236	14.015565	-0.061350	4.815414
301.836257	7999.956319	14.020570	-0.061353	4.815340
301.885109	7999.995616	14.025575	-0.061363	4.815352
301.812610	8000.177212	14.030579	-0.061349	4.815405
301.862704	7999.996315	14.035584	-0.061358	4.815352
301.721910	8000.131879	14.040589	-0.061332	4.815392
301.861126	8000.109606	14.045594	-0.061358	4.815385
302.074962	8000.025500	14.050599	-0.061398	4.815360
302.059179	8000.208040	14.055603	-0.061395	4.815413
302.022206	7999.955142	14.060608	-0.061388	4.815339
301.958166	8000.407340	14.065613	-0.061377	4.815472
302.044101	8000.218484	14.070618	-0.061392	4.815416
301.981051	8000.215300	14.075623	-0.061381	4.815415
301.983434	8000.424869	14.080627	-0.061381	4.815477
302.101928	8000.072994	14.085632	-0.061403	4.815373
301.846284	8000.117923	14.090637	-0.061356	4.815388
301.721148	8000.166089	14.095642	-0.061332	4.815402
301.918734	8000.053920	14.100647	-0.061369	4.815369
301.871384	8000.176070	14.105651	-0.061360	4.815404
301.860242	8000.215440	14.110656	-0.061358	4.815416
301.832124	8000.209629	14.115661	-0.061353	4.815414
301.787509	8000.104127	14.120666	-0.061345	4.815384
301.882670	8000.116399	14.125671	-0.061363	4.815387
301.882410	8000.257505	14.130675	-0.061363	4.815428
301.942972	8000.162301	14.135680	-0.061374	4.815400
301.872730	8000.350351	14.140685	-0.061361	4.815455
302.039737	8000.224845	14.145690	-0.061392	4.815418
302.059612	8000.339562	14.150695	-0.061396	4.815451
301.755552	8000.444620	14.155699	-0.061339	4.815483
302.010423	8000.290641	14.160704	-0.061387	4.815437
301.877447	8000.355782	14.165709	-0.061362	4.815457
302.047396	8000.437715	14.170714	-0.061394	4.815480
301.969788	8000.155274	14.175719	-0.061379	4.815398
301.919462	8000.124507	14.180723	-0.061370	4.815389
302.022729	8000.260920	14.185728	-0.061389	4.815429
301.895509	8000.440541	14.190733	-0.061365	4.815482
302.016971	8000.266172	14.195738	-0.061388	4.815430
302.027478	8000.167998	14.200743	-0.061390	4.815401
302.098455	8000.293185	14.205747	-0.061403	4.815438
302.077418	8000.150657	14.210752	-0.061399	4.815396
302.000641	8000.274458	14.215757	-0.061385	4.815433
301.930410	8000.242291	14.220762	-0.061372	4.815424
301.960977	8000.131623	14.225767	-0.061377	4.815391
301.877906	8000.227524	14.230771	-0.061362	4.815419
302.040714	8000.044223	14.235776	-0.061392	4.815365
301.971572	8000.299638	14.240781	-0.061380	4.815440
301.765787	8000.111282	14.245786	-0.061341	4.815386
302.020239	8000.226687	14.250791	-0.061389	4.815419
301.903984	8000.185204	14.255795	-0.061367	4.815407
301.944374	7999.550895	14.260800	-0.061374	4.815222
301.964734	7996.263409	14.265805	-0.061376	4.814261
302.078087	7990.703328	14.270810	-0.061393	4.812636
301.986237	7983.980852	14.275815	-0.061372	4.810672
301.785844	7976.638133	14.280819	-0.061330	4.808526
301.882689	7969.028201	14.285824	-0.061343	4.806299
301.740619	7961.227124	14.290829	-0.061311	4.804017
301.681579	7953.296790	14.295834	-0.061295	4.801695
301.823490	7945.386179	14.300839	-0.061316	4.799377
301.627591	7937.395444	14.305843	-0.061275	4.797036
301.758879	7929.421017	14.310848	-0.061294	4.794697
301.651662	7921.370334	14.315853	-0.061269	4.792335
301.766636	7913.386441	14.320858	-0.061285	4.789991
301.786859	7905.407190	14.325863	-0.061284	4.787648
301.462705	7897.383429	14.330867	-0.061218	4.785292
301.657538	7889.427254	14.335872	-0.061249	4.782952
301.699157	7881.428230	14.340877	-0.061252	4.780599
301.654303	7873.404387	14.345882	-0.061238	4.778238
301.666647	7865.430887	14.350887	-0.061235	4.775891
301.665614	7857.372123	14.355891	-0.061230	4.773517
301.415325	7849.352274	14.360896	-0.061178	4.771155
301.183545	7841.381201	14.365901	-0.061130	4.768805
301.228711	7833.334045	14.370906	-0.061133	4.766432
301.262318	7825.385928	14.375911	-0.061134	4.764086
301.282242	7817.387645	14.380915	-0.061132	4.761724
301.288714	7809.347739	14.385920	-0.061128	4.759349
301.345785	7801.394818	14.390925	-0.061134	4.756998
301.197480	7793.302000	14.395930	-0.061101	4.754605
301.235588	7785.303007	14.400935	-0.061103	4.752238
300.948129	7777.259003	14.405939	-0.061044	4.749858
301.072833	7769.354371	14.410944	-0.061062	4.747517
300.882050	7761.294289	14.415949	-0.061021	4.745129
300.810876	7753.357533	14.420954	-0.061003	4.742776
300.958759	7745.304971	14.425959	-0.061025	4.740387
300.984326	7737.296187	14.430963	-0.061025	4.738010
301.003509	7729.352327	14.435968	-0.061023	4.735652
300.917045	7721.270591	14.440973	-0.061002	4.733251
300.702199	7713.244264	14.445978	-0.060957	4.730866
300.747142	7705.343144	14.450983	-0.060960	4.728517
300.595806	7697.300394	14.455987	-0.060927	4.726124
300.538410	7689.304579	14.460992	-0.060911	4.723744
300.560666	7681.320868	14.465997	-0.060910	4.721367
300.480859	7673.291059	14.471002	-0.060890	4.718974
300.541824	7665.393242	14.476007	-0.060896	4.716620
300.369154	7657.263008	14.481011	-0.060858	4.714195
300.468597	7649.262657	14.486016	-0.060872	4.711807
300.542922	7641.282859	14.491021	-0.060880	4.709425
300.337585	7633.264169	14.496026	-0.060837	4.707030
300.371959	7625.269207	14.501031	-0.060838	4.704640
300.405987	7617.298132	14.506035	-0.060839	4.702257
300.313105	7609.275938	14.511040	-0.060817	4.699857
300.299675	7601.346026	14.516045	-0.060809	4.697483
300.355902	7593.297629	14.521050	-0.060814	4.695073
300.392367	7585.281347	14.526055	-0.060816	4.692670
300.342362	7577.194694	14.531059	-0.060801	4.690246
300.330393	7569.303951	14.536064	-0.060794	4.687879
300.475933	7561.269421	14.541069	-0.060816	4.685468
300.207017	7553.339492	14.546074	-0.060761	4.683087
300.286566	7545.311759	14.551079	-0.060770	4.680676
300.118419	7537.251496	14.556083	-0.060734	4.678253
300.334686	7529.279478	14.561088	-0.060769	4.675856
300.049367	7521.178251	14.566093	-0.060710	4.673419
300.130243	7513.138085	14.571098	-0.060720	4.670998
300.071147	7505.223699	14.576103	-0.060704	4.668614
299.887344	7497.197864	14.581107	-0.060665	4.666196
299.918280	7489.256890	14.586112	-0.060665	4.663802
299.999006	7481.207412	14.591117	-0.060675	4.661374
300.017263	7473.236324	14.596122	-0.060673	4.658968
300.047244	7465.291103	14.601127	-0.060674	4.656569
299.901314	7457.193371	14.606131	-0.060641	4.654122
299.864287	7449.208733	14.611136	-0.060629	4.651709
299.629281	7441.193597	14.616141	-0.060580	4.649285
299.602781	7433.180247	14.621146	-0.060570	4.646860
299.819098	7425.178967	14.626151	-0.060605	4.644437
299.634541	7417.248792	14.631155	-0.060566	4.642035
299.576654	7409.191274	14.636160	-0.060550	4.639593
299.610854	7401.313202	14.641165	-0.060551	4.637204
299.536793	7393.198250	14.646170	-0.060532	4.634742
299.648908	7385.192844	14.651175	-0.060547	4.632312
299.594610	7377.127635	14.656179	-0.060532	4.629862
299.543705	7369.163277	14.661184	-0.060517	4.627442
299.274134	7361.136139	14.666189	-0.060462	4.625002
299.422208	7353.200956	14.671194	-0.060484	4.622588
299.669759	7345.175599	14.676199	-0.060525	4.620145
299.336160	7337.245295	14.681203	-0.060458	4.617730
299.254902	7329.188244	14.686208	-0.060438	4.615275
299.289246	7321.186733	14.691213	-0.060439	4.612836
299.239340	7313.116796	14.696218	-0.060424	4.610375
299.279443	7305.184137	14.701223	-0.060427	4.607954
299.401657	7297.107382	14.706227	-0.060444	4.605488
299.352977	7289.203596	14.711232	-0.060430	4.603073
299.204691	7281.165187	14.716237	-0.060397	4.600616
299.009007	7273.195484	14.721242	-0.060355	4.598179
299.095085	7265.196094	14.726247	-0.060366	4.595731
299.000094	7257.088027	14.731251	-0.060343	4.593249
298.975521	7249.093304	14.736256	-0.060334	4.590800
299.152345	7241.095381	14.741261	-0.060361	4.588349
298.843189	7233.112803	14.746266	-0.060299	4.585901
298.868879	7225.173569	14.751271	-0.060298	4.583465
298.868615	7217.119653	14.756275	-0.060293	4.580993
299.005858	7209.142911	14.761280	-0.060313	4.578543
298.899174	7201.134497	14.766285	-0.060288	4.576082
298.899747	7193.088507	14.771290	-0.060283	4.573608
298.889989	7185.097639	14.776295	-0.060276	4.571150
298.621313	7177.098759	14.781299	-0.060221	4.568688
298.540961	7169.104656	14.786304	-0.060201	4.566226
298.667174	7161.113126	14.791309	-0.060219	4.563763
298.659350	7153.101081	14.796314	-0.060212	4.561293
298.463535	7145.176115	14.801319	-0.060171	4.558848
298.271724	7137.155351	14.806323	-0.060130	4.556373
298.408708	7129.125428	14.811328	-0.060150	4.553893
298.307667	7121.114078	14.816333	-0.060126	4.551418
298.395383	7113.080975	14.821338	-0.060137	4.548934
298.588113	7105.097109	14.826343	-0.060168	4.546465
298.535979	7097.072408	14.831347	-0.060153	4.543982
298.406376	7089.130160	14.836352	-0.060124	4.541522
298.198906	7081.122192	14.841357	-0.060080	4.539041
298.504144	7073.119728	14.846362	-0.060131	4.536561
298.282857	7065.114641	14.851367	-0.060085	4.534077
298.319190	7057.039011	14.856371	-0.060087	4.531571
298.321356	7049.091701	14.861376	-0.060082	4.529104
298.324032	7041.103517	14.866381	-0.060077	4.526622
298.174217	7033.067541	14.871386	-0.060044	4.524124
298.284663	7025.149657	14.876391	-0.060059	4.521661
297.974673	7017.068567	14.881395	-0.059996	4.519146
297.943641	7009.152438	14.886400	-0.059986	4.516681
297.939818	7001.075135	14.891405	-0.059980	4.514165
297.815681	6992.978249	14.896410	-0.059951	4.511641
297.879988	6985.031560	14.901415	-0.059958	4.509163
297.828434	6977.013153	14.906419	-0.059943	4.506660
297.897840	6969.039202	14.911424	-0.059951	4.504171
297.846024	6961.095654	14.916429	-0.059936	4.501689
297.644504	6953.041995	14.921434	-0.059893	4.499171
297.664153	6945.084763	14.926439	-0.059892	4.496683
297.670496	6937.029325	14.931443	-0.059888	4.494162
297.643858	6929.040525	14.936448	-0.059878	4.491661
297.677229	6921.032707	14.941453	-0.059879	4.489152
297.751201	6913.019009	14.946458	-0.059887	4.486640
297.650422	6905.045345	14.951463	-0.059863	4.484139
297.388054	6897.085766	14.956467	-0.059809	4.481641
297.379445	6889.020766	14.961472	-0.059802	4.479109
297.420835	6881.101885	14.966477	-0.059805	4.476621
297.444486	6872.996942	14.971482	-0.059804	4.474073
297.480808	6865.021515	14.976487	-0.059806	4.471565
297.438904	6857.030595	14.981491	-0.059793	4.469050
297.324275	6849.024200	14.986496	-0.059766	4.466529
297.287474	6841.027432	14.991501	-0.059754	4.464010
297.321867	6833.034372	14.996506	-0.059755	4.461490
297.385148	6825.036573	15.001511	-0.059762	4.458968
297.348735	6817.033604	15.006515	-0.059750	4.456442
297.079540	6809.026180	15.011520	-0.059695	4.453913
297.138206	6800.991684	15.016525	-0.059700	4.451375
297.158499	6792.992848	15.021530	-0.059699	4.448846
297.125236	6785.003193	15.026535	-0.059687	4.446319
297.130927	6777.006746	15.031539	-0.059683	4.443788
297.137998	6768.998087	15.036544	-0.059679	4.441252
297.066771	6761.016728	15.041549	-0.059661	4.438723
296.987093	6753.009549	15.046554	-0.059641	4.436184
296.953532	6745.015213	15.051559	-0.059630	4.433648
296.861290	6736.937790	15.056563	-0.059607	4.431084
296.892669	6728.944908	15.061568	-0.059608	4.428546
297.048243	6720.947945	15.066573	-0.059632	4.426006
296.804184	6712.944648	15.071578	-0.059581	4.423460
296.963842	6704.978371	15.076583	-0.059605	4.420926
296.772149	6696.983615	15.081587	-0.059565	4.418381
296.854741	6688.969799	15.086592	-0.059575	4.415829
296.807287	6680.970421	15.091597	-0.059561	4.413279
296.964543	6672.934339	15.096602	-0.059585	4.410718
296.895837	6664.973923	15.101607	-0.059567	4.408178
296.590288	6656.948572	15.106611	-0.059505	4.405614
296.619914	6648.985159	15.111616	-0.059505	4.403071
296.695257	6640.976771	15.116621	-0.059514	4.400512
296.451781	6633.016342	15.121626	-0.059463	4.397965
296.498933	6625.007983	15.126631	-0.059467	4.395402
296.330739	6616.916283	15.131635	-0.059430	4.392811
296.525567	6608.894357	15.136640	-0.059461	4.390242
296.426103	6600.963929	15.141645	-0.059438	4.387699
296.310824	6592.926511	15.146650	-0.059411	4.385121
296.472474	6585.004720	15.151655	-0.059436	4.382580
296.405628	6576.954494	15.156659	-0.059418	4.379994
296.310896	6569.019330	15.161664	-0.059395	4.377444
296.608979	6560.995267	15.166669	-0.059446	4.374866
296.297992	6552.996749	15.171674	-0.059383	4.372292
296.350896	6544.954601	15.176679	-0.059387	4.369704
296.199301	6536.978231	15.181683	-0.059354	4.367134
296.288906	6528.951675	15.186688	-0.059365	4.364548
296.156449	6521.046397	15.191693	-0.059336	4.361998
295.884363	6512.966639	15.196698	-0.059280	4.359390
296.241224	6505.020668	15.201703	-0.059341	4.356827
295.927463	6496.946601	15.206707	-0.059277	4.354217
295.820195	6488.835724	15.211712	-0.059252	4.351595
295.996548	6480.890059	15.216717	-0.059280	4.349026
295.655458	6472.921948	15.221722	-0.059211	4.346446
295.776123	6464.943435	15.226727	-0.059228	4.343863
295.743148	6456.939099	15.231731	-0.059217	4.341270
295.807682	6448.934636	15.236736	-0.059224	4.338675
295.715143	6440.971940	15.241741	-0.059201	4.336092
295.717833	6432.927380	15.246746	-0.059197	4.333481
295.762957	6424.922321	15.251751	-0.059200	4.330882
295.641704	6416.937197	15.256755	-0.059172	4.328286
295.591847	6408.950555	15.261760	-0.059158	4.325689
295.692293	6400.948147	15.266765	-0.059171	4.323086
295.486534	6392.915172	15.271770	-0.059128	4.320469
295.337290	6385.000859	15.276775	-0.059095	4.317890
295.323787	6376.912070	15.281779	-0.059087	4.315254
295.260610	6368.913589	15.286784	-0.059070	4.312645
295.263322	6360.892638	15.291789	-0.059065	4.310027
295.319526	6352.903040	15.296794	-0.059070	4.307419
295.600512	6344.928277	15.301799	-0.059118	4.304815
295.327397	6336.925518	15.306803	-0.059062	4.302197
295.219965	6328.936201	15.311808	-0.059036	4.299582
295.340010	6320.993045	15.316813	-0.059054	4.296983
295.422391	6312.882137	15.321818	-0.059064	4.294328
295.297710	6304.926034	15.326823	-0.059035	4.291719
295.272130	6296.881970	15.331827	-0.059025	4.289081
295.346838	6288.912671	15.336832	-0.059034	4.286467
295.207479	6280.950716	15.341837	-0.059003	4.283851
294.946979	6272.906491	15.346842	-0.058949	4.281206
295.126851	6264.943509	15.351847	-0.058977	4.278590
295.154278	6256.904789	15.356851	-0.058977	4.275946
295.026302	6248.864616	15.361856	-0.058948	4.273299
295.083338	6240.869218	15.366861	-0.058954	4.270666
294.826392	6232.857594	15.371866	-0.058901	4.268023
294.862434	6224.939857	15.376871	-0.058902	4.265413
294.753711	6216.922976	15.381875	-0.058877	4.262767
295.055576	6208.873670	15.386880	-0.058928	4.260112
294.924328	6200.944858	15.391885	-0.058898	4.257491
294.820519	6192.886178	15.396890	-0.058874	4.254826
294.682940	6184.879754	15.401895	-0.058843	4.252176
294.645618	6176.867136	15.406899	-0.058831	4.249524
294.469656	6168.869043	15.411904	-0.058793	4.246873
294.657544	6160.906358	15.416909	-0.058822	4.244236
294.731533	6152.902815	15.421914	-0.058831	4.241583
294.541147	6144.931494	15.426919	-0.058790	4.238936
294.385673	6136.933222	15.431923	-0.058756	4.236279
294.623048	6128.888373	15.436928	-0.058795	4.233608
294.701046	6120.832462	15.441933	-0.058804	4.230931
294.516445	6112.869949	15.446938	-0.058765	4.228280
294.422151	6104.907055	15.451943	-0.058742	4.225629
294.313566	6096.955248	15.456947	-0.058717	4.222979
294.258817	6088.899197	15.461952	-0.058701	4.220294
294.301315	6080.940855	15.466957	-0.058704	4.217640
294.291766	6072.874978	15.471962	-0.058697	4.214948
294.304333	6064.927622	15.476967	-0.058694	4.212294
294.276716	6056.889358	15.481971	-0.058684	4.209608
294.134019	6048.923244	15.486976	-0.058652	4.206943
294.276909	6040.912394	15.491981	-0.058674	4.204265
294.097442	6032.950160	15.496986	-0.058635	4.201597
294.189201	6024.966896	15.501991	-0.058647	4.198924
294.213241	6016.930293	15.506995	-0.058646	4.196230
293.989264	6008.870397	15.512000	-0.058599	4.193524
293.952867	6000.818208	15.517005	-0.058587	4.190821
293.789786	5992.837550	15.522010	-0.058552	4.188139
293.839010	5984.896107	15.527015	-0.058556	4.185471
293.747445	5976.894668	15.532019	-0.058533	4.182779
293.750434	5968.884216	15.537024	-0.058529	4.180083
293.849769	5960.899880	15.542029	-0.058542	4.177396
293.586754	5952.877940	15.547034	-0.058488	4.174690
293.593185	5944.894966	15.552039	-0.058484	4.171999
293.749395	5936.858499	15.557043	-0.058508	4.169289
293.513069	5928.898607	15.562048	-0.058459	4.166599
293.661223	5920.903274	15.567053	-0.058481	4.163900
293.584724	5912.893919	15.572058	-0.058461	4.161192
293.519949	5904.925401	15.577063	-0.058444	4.158495
293.615970	5896.892025	15.582067	-0.058457	4.155777
293.645340	5888.867093	15.587072	-0.058457	4.153060
293.592933	5880.860376	15.592077	-0.058442	4.150345
293.356866	5872.879138	15.597082	-0.058393	4.147636
293.335776	5864.832222	15.602087	-0.058384	4.144905
293.249377	5856.904133	15.607091	-0.058363	4.142211
293.295234	5848.869096	15.612096	-0.058366	4.139482
293.314047	5840.896299	15.617101	-0.058364	4.136771
293.211612	5832.864285	15.622106	-0.058340	4.134036
293.351443	5824.859148	15.627111	-0.058361	4.131312
293.388752	5816.871201	15.632115	-0.058363	4.128591
293.346187	5808.844737	15.637120	-0.058349	4.125854
293.456173	5800.915920	15.642125	-0.058365	4.123151
293.193458	5792.890802	15.647130	-0.058311	4.120408
293.135331	5784.946705	15.652135	-0.058295	4.117693
293.151321	5776.874565	15.657139	-0.058292	4.114934
292.919012	5768.829902	15.662144	-0.058244	4.112179
293.109608	5760.849594	15.667149	-0.058274	4.109450
293.200552	5752.837282	15.672154	-0.058286	4.106706
293.039958	5744.857149	15.677159	-0.058251	4.103969
292.921299	5736.834407	15.682163	-0.058224	4.101216
292.799031	5728.869987	15.687168	-0.058196	4.098481
292.957431	5720.896482	15.692173	-0.058220	4.095744
292.755739	5712.876824	15.697178	-0.058177	4.092985
292.752428	5704.884882	15.702183	-0.058171	4.090237
292.856516	5696.912253	15.707187	-0.058186	4.087494
292.879627	5688.879250	15.712192	-0.058185	4.084728
292.733148	5680.938088	15.717197	-0.058152	4.081990
292.654716	5672.881965	15.722202	-0.058132	4.079210
292.907405	5664.923065	15.727207	-0.058174	4.076467
292.783325	5656.914947	15.732211	-0.058146	4.073700
292.527180	5648.868880	15.737216	-0.058093	4.070916
292.612527	5640.913881	15.742221	-0.058104	4.068167
292.445363	5632.887020	15.747226	-0.058067	4.065387
292.313026	5624.985079	15.752231	-0.058038	4.062649
292.339931	5616.908147	15.757235	-0.058037	4.059851
292.258067	5608.919577	15.762240	-0.058017	4.057080
292.278503	5600.939460	15.767245	-0.058016	4.054311
292.252074	5592.898432	15.772250	-0.058005	4.051519
292.208324	5584.896028	15.777255	-0.057992	4.048738
292.162549	5576.933342	15.782259	-0.057978	4.045968
292.109203	5568.940574	15.787264	-0.057963	4.043187
292.049632	5560.922226	15.792269	-0.057947	4.040394
291.898954	5552.938420	15.797274	-0.057914	4.037610
292.076799	5544.918372	15.802279	-0.057942	4.034817
292.048507	5536.825911	15.807283	-0.057931	4.031993
292.011353	5528.832486	15.812288	-0.057919	4.029201
291.948750	5520.879672	15.817293	-0.057902	4.026422
291.972277	5512.862571	15.822298	-0.057901	4.023619
292.093976	5504.902952	15.827303	-0.057919	4.020836
292.042294	5496.928793	15.832307	-0.057904	4.018044
291.830938	5488.871057	15.837312	-0.057859	4.015217
291.966549	5480.911402	15.842317	-0.057879	4.012429
291.755838	5472.833899	15.847322	-0.057835	4.009592
291.849606	5464.897915	15.852327	-0.057847	4.006807
291.884069	5456.899908	15.857331	-0.057849	4.003997
291.701028	5448.933305	15.862336	-0.057809	4.001193
291.728214	5440.918487	15.867341	-0.057809	3.998374
291.625807	5432.908127	15.872346	-0.057785	3.995552
291.703167	5424.899685	15.877351	-0.057794	3.992731
291.329839	5416.898101	15.882355	-0.057719	3.989904
291.412554	5408.871591	15.887360	-0.057730	3.987073
291.546866	5400.916423	15.892365	-0.057749	3.984267
291.439646	5392.933881	15.897370	-0.057724	3.981444
291.365920	5384.925478	15.902375	-0.057705	3.978612
291.341920	5376.924012	15.907379	-0.057696	3.975780
291.433487	5368.891094	15.912384	-0.057707	3.972937
291.384855	5360.898706	15.917389	-0.057693	3.970104
291.220543	5352.925463	15.922394	-0.057657	3.967274
291.153897	5344.907597	15.927399	-0.057640	3.964428
291.147036	5336.979669	15.932403	-0.057633	3.961612
291.294223	5328.961285	15.937408	-0.057656	3.958765
291.313024	5320.976747	15.942413	-0.057654	3.955926
291.209522	5312.927570	15.947418	-0.057629	3.953060
291.022450	5304.922522	15.952423	-0.057589	3.950206
290.871288	5296.934728	15.957427	-0.057556	3.947356
290.871539	5288.905973	15.962432	-0.057551	3.944493
290.874923	5280.977337	15.967437	-0.057546	3.941663
290.870916	5272.952534	15.972442	-0.057540	3.938797
290.814398	5264.967618	15.977447	-0.057525	3.935942
290.611219	5256.968782	15.982451	-0.057482	3.933077
290.489959	5248.933411	15.987456	-0.057454	3.930198
290.705264	5240.989028	15.992461	-0.057489	3.927356
290.728110	5232.926806	15.997466	-0.057488	3.924467
290.660551	5224.997754	16.002471	-0.057470	3.921621
290.494486	5217.001255	16.007475	-0.057434	3.918747
290.519190	5208.984474	16.012480	-0.057433	3.915867
290.574223	5200.970299	16.017485	-0.057438	3.912987
290.301689	5192.936326	16.022490	-0.057382	3.910091
290.472768	5184.947969	16.027495	-0.057409	3.907218
290.283518	5176.958945	16.032499	-0.057369	3.904336
290.058916	5169.002842	16.037504	-0.057322	3.901463
290.268473	5161.009319	16.042509	-0.057355	3.898582
290.207548	5152.981329	16.047514	-0.057339	3.895682
290.114788	5144.984336	16.052519	-0.057316	3.892790
290.094146	5136.951565	16.057523	-0.057307	3.889884
290.094982	5128.965063	16.062528	-0.057302	3.886994
290.455983	5120.951604	16.067533	-0.057364	3.884098
290.187085	5112.993892	16.072538	-0.057309	3.881208
290.315097	5105.012401	16.077543	-0.057328	3.878315
290.304542	5096.994393	16.082547	-0.057321	3.875404
290.193466	5088.773940	16.087552	-0.057294	3.872416
290.256140	5080.807143	16.092557	-0.057301	3.869520
289.900204	5072.888726	16.097562	-0.057230	3.866632
289.970519	5064.887183	16.102567	-0.057237	3.863720
289.785928	5056.951823	16.107571	-0.057198	3.860825
289.739422	5048.950747	16.112576	-0.057184	3.857906
289.782843	5040.953370	16.117581	-0.057187	3.854988
289.745987	5032.934854	16.122586	-0.057175	3.852059
289.797995	5024.968765	16.127591	-0.057179	3.849148
289.924555	5016.967854	16.132595	-0.057198	3.846224
289.681098	5008.972312	16.137600	-0.057147	3.843292
289.559646	5001.036634	16.142605	-0.057119	3.840382
289.577171	4993.020058	16.147610	-0.057118	3.837444
289.668518	4985.012264	16.152615	-0.057129	3.834507
289.542708	4977.004158	16.157619	-0.057101	3.831564
289.820241	4968.960687	16.162624	-0.057147	3.828614
289.755984	4961.008962	16.167629	-0.057130	3.825689
289.448712	4953.019579	16.172634	-0.057068	3.822742
289.400370	4945.026733	16.177639	-0.057053	3.819797
289.424558	4937.082470	16.182643	-0.057053	3.816869
289.304628	4929.056177	16.187648	-0.057025	3.813906
289.490913	4921.057328	16.192653	-0.057055	3.810957
289.552458	4913.031302	16.197658	-0.057061	3.807993
289.420820	4905.071722	16.202663	-0.057031	3.805047
289.271865	4897.082275	16.207667	-0.056998	3.802087
289.461905	4889.073323	16.212672	-0.057029	3.799125
289.435754	4881.095062	16.217677	-0.057018	3.796168
289.095104	4873.083561	16.222682	-0.056950	3.793189
289.058693	4865.050386	16.227687	-0.056938	3.790206
289.059231	4857.051602	16.232691	-0.056933	3.787234
289.017055	4849.018841	16.237696	-0.056920	3.784247
289.104668	4841.119715	16.242701	-0.056931	3.781310
289.100386	4833.061246	16.247706	-0.056925	3.778309
288.995875	4825.098128	16.252711	-0.056900	3.775339
288.900727	4817.102273	16.257715	-0.056877	3.772355
288.850058	4809.033176	16.262720	-0.056863	3.769342
289.052544	4801.091334	16.267725	-0.056895	3.766379
289.040073	4793.066935	16.272730	-0.056888	3.763379
288.699253	4785.119090	16.277735	-0.056819	3.760398
288.768941	4777.124160	16.282739	-0.056827	3.757405
288.698932	4769.094214	16.287744	-0.056808	3.754395
288.762680	4761.089941	16.292749	-0.056815	3.751394
288.729169	4753.059002	16.297754	-0.056804	3.748379
288.824745	4745.070549	16.302759	-0.056816	3.745380
288.579067	4737.125515	16.307763	-0.056765	3.742387
288.522757	4729.111237	16.312768	-0.056750	3.739371
288.635468	4721.174895	16.317773	-0.056766	3.736385
288.437581	4713.123635	16.322778	-0.056723	3.733346
288.421359	4705.093201	16.327783	-0.056715	3.730316
288.629323	4697.120415	16.332787	-0.056749	3.727312
288.363486	4689.081645	16.337792	-0.056694	3.724269
288.454374	4681.190260	16.342797	-0.056706	3.721287
288.322310	4673.172618	16.347802	-0.056676	3.718250
288.453891	4665.166937	16.352807	-0.056695	3.715221
288.350314	4657.079110	16.357811	-0.056671	3.712153
288.008632	4649.093181	16.362816	-0.056602	3.709116
288.039822	4641.109555	16.367821	-0.056603	3.706085
287.990519	4633.144245	16.372826	-0.056588	3.703058
287.833375	4625.151462	16.377831	-0.056554	3.700014
288.031809	4617.192140	16.382835	-0.056586	3.696990
288.024082	4609.151972	16.387840	-0.056579	3.693927
287.910285	4601.192573	16.392845	-0.056553	3.690890
287.993201	4593.183476	16.397850	-0.056563	3.687837
287.969440	4585.158607	16.402855	-0.056553	3.684772
288.017054	4577.220628	16.407859	-0.056557	3.681739
287.945560	4569.165725	16.412864	-0.056538	3.678657
287.971995	4561.230925	16.417869	-0.056538	3.675620
287.727187	4553.201878	16.422874	-0.056487	3.672538
287.804561	4545.174372	16.427879	-0.056496	3.669461
287.846095	4537.221845	16.432883	-0.056499	3.666411
287.672532	4529.196986	16.437888	-0.056461	3.663324
287.528861	4521.262193	16.442893	-0.056430	3.660270
287.490695	4513.258805	16.447898	-0.056417	3.657190
287.661425	4505.213132	16.452903	-0.056444	3.654096
287.786024	4497.218646	16.457907	-0.056462	3.651019
287.505707	4489.207563	16.462912	-0.056404	3.647921
287.547364	4481.227417	16.467917	-0.056407	3.644842
287.510794	4473.254536	16.472922	-0.056395	3.641760
287.435474	4465.282219	16.477927	-0.056376	3.638675
287.439913	4457.269258	16.482931	-0.056371	3.635574
287.407371	4449.238312	16.487936	-0.056360	3.632463
287.236525	4441.238372	16.492941	-0.056323	3.629357
287.155407	4433.238303	16.497946	-0.056303	3.626250
287.389033	4425.231964	16.502951	-0.056341	3.623147
287.270207	4417.279577	16.507955	-0.056314	3.620053
287.089197	4409.301518	16.512960	-0.056275	3.616944
287.268664	4401.296978	16.517965	-0.056303	3.613833
287.163389	4393.275342	16.522970	-0.056278	3.610704
286.968749	4385.314253	16.527975	-0.056237	3.607593
287.116239	4377.276649	16.532979	-0.056259	3.604460
287.093253	4369.330009	16.537984	-0.056250	3.601354
286.920985	4361.384148	16.542989	-0.056212	3.598242
286.621469	4353.357089	16.547994	-0.056151	3.595092
286.862303	4345.311923	16.552999	-0.056191	3.591947
287.026967	4337.307842	16.558003	-0.056217	3.588814
286.849181	4329.321902	16.563008	-0.056178	3.585675
286.752100	4321.376922	16.568013	-0.056155	3.582552
286.604531	4313.350501	16.573018	-0.056122	3.579392
286.579124	4305.414347	16.578023	-0.056112	3.576269
286.741986	4297.400870	16.583027	-0.056138	3.573118
286.652154	4289.338469	16.588032	-0.056116	3.569938
286.630456	4281.397744	16.593037	-0.056106	3.566804
286.658542	4273.395541	16.598042	-0.056106	3.563646
286.598155	4265.400636	16.603047	-0.056090	3.560484
286.776693	4257.451994	16.608051	-0.056118	3.557345
286.621016	4249.384528	16.613056	-0.056084	3.554147
286.509598	4241.314022	16.618061	-0.056058	3.550946
286.517720	4233.356812	16.623066	-0.056054	3.547790
286.446379	4225.363098	16.628071	-0.056036	3.544614
286.259849	4217.442552	16.633075	-0.055996	3.541462
286.388101	4209.407410	16.638080	-0.056014	3.538270
286.504612	4201.425821	16.643085	-0.056031	3.535097
286.091859	4193.408296	16.648090	-0.055949	3.531890
286.207313	4185.391902	16.653095	-0.055965	3.528697
286.187193	4177.434446	16.658099	-0.055956	3.525520
286.056790	4169.458981	16.663104	-0.055927	3.522330
286.048454	4161.465884	16.668109	-0.055920	3.519134
286.212931	4153.455143	16.673114	-0.055946	3.515933
286.122015	4145.462643	16.678119	-0.055923	3.512729
286.130979	4137.451904	16.683123	-0.055920	3.509517
285.882806	4129.463651	16.688128	-0.055868	3.506303
285.905327	4121.486785	16.693133	-0.055867	3.503100
285.712488	4113.505174	16.698138	-0.055826	3.499885
285.806788	4105.529631	16.703143	-0.055839	3.496678
285.738221	4097.536858	16.708147	-0.055821	3.493457
285.615211	4089.492274	16.713152	-0.055793	3.490209
285.771179	4081.554819	16.718157	-0.055817	3.487011
285.803195	4073.530004	16.723162	-0.055817	3.483771
285.731455	4065.545501	16.728167	-0.055799	3.480541
285.524744	4057.619957	16.733171	-0.055755	3.477327
285.583767	4049.558349	16.738176	-0.055761	3.474063
285.666107	4041.549398	16.743181	-0.055771	3.470819
285.294639	4033.570090	16.748186	-0.055697	3.467569
285.347965	4025.556950	16.753191	-0.055701	3.464316
285.629146	4017.601449	16.758195	-0.055749	3.461091
285.516090	4009.587382	16.763200	-0.055722	3.457826
285.454376	4001.605171	16.768205	-0.055706	3.454572
285.306934	3993.609849	16.773210	-0.055673	3.451307
285.295884	3985.591299	16.778215	-0.055666	3.448035
285.106890	3977.611545	16.783219	-0.055625	3.444769
285.176618	3969.635302	16.788224	-0.055633	3.441510
285.278561	3961.654061	16.793229	-0.055647	3.438247
285.093808	3953.652634	16.798234	-0.055607	3.434963
285.258257	3945.635050	16.803239	-0.055633	3.431680
285.279747	3937.645869	16.808243	-0.055632	3.428402
285.212943	3929.620668	16.813248	-0.055614	3.425103
284.989479	3921.691218	16.818253	-0.055567	3.421834
285.041622	3913.686885	16.823258	-0.055572	3.418541
284.926794	3905.685085	16.828263	-0.055545	3.415240
284.846396	3897.696555	16.833267	-0.055525	3.411943
284.714001	3889.676258	16.838272	-0.055495	3.408627
284.828460	3881.719596	16.843277	-0.055511	3.405343
284.697212	3873.760841	16.848282	-0.055482	3.402047
284.663253	3865.752759	16.853287	-0.055470	3.398730
284.736578	3857.796999	16.858291	-0.055478	3.395435
284.749439	3849.668208	16.863296	-0.055476	3.392063
284.597479	3841.691348	16.868301	-0.055442	3.388746
284.472583	3833.729106	16.873306	-0.055414	3.385432
284.805674	3825.733061	16.878311	-0.055471	3.382116
284.866286	3817.786490	16.883315	-0.055477	3.378809
284.422157	3809.803654	16.888320	-0.055389	3.375465
284.538412	3801.797760	16.893325	-0.055405	3.372128
284.355995	3793.810245	16.898330	-0.055366	3.368785
284.401315	3785.794139	16.903335	-0.055369	3.365435
284.635355	3777.833965	16.908339	-0.055408	3.362112
284.454745	3769.838916	16.913344	-0.055369	3.358756
284.570396	3761.878565	16.918349	-0.055385	3.355421
284.564810	3753.825768	16.923354	-0.055379	3.352041
284.478345	3745.826700	16.928359	-0.055358	3.348676
284.350866	3737.868938	16.933363	-0.055329	3.345324
284.311311	3729.873055	16.938368	-0.055316	3.341956
284.343161	3721.887934	16.943373	-0.055317	3.338591
283.991932	3713.919820	16.948378	-0.055246	3.335216
283.966662	3705.907101	16.953383	-0.055236	3.331831
284.199703	3697.902817	16.958387	-0.055275	3.328455
283.975600	3689.909036	16.963392	-0.055228	3.325064
284.142824	3681.944367	16.968397	-0.055254	3.321696
284.019844	3673.958815	16.973402	-0.055226	3.318305
284.013288	3665.966066	16.978407	-0.055219	3.314912
284.061476	3657.961244	16.983411	-0.055223	3.311512
283.904895	3649.949772	16.988416	-0.055189	3.308098
283.931902	3641.941327	16.993421	-0.055188	3.304689
283.810806	3634.008496	16.998426	-0.055161	3.301302
283.668620	3626.016278	17.003431	-0.055129	3.297887
283.671079	3618.015092	17.008435	-0.055124	3.294469
283.613467	3610.013731	17.013440	-0.055108	3.291045
283.595732	3602.041202	17.018445	-0.055100	3.287632
283.373504	3594.072799	17.023450	-0.055053	3.284209
283.390816	3586.072290	17.028455	-0.055051	3.280778
283.343559	3578.106331	17.033459	-0.055037	3.277356
283.226434	3570.079553	17.038464	-0.055010	3.273901
283.236421	3562.053392	17.043469	-0.055007	3.270448
283.231403	3554.070396	17.048474	-0.055001	3.267009
283.188244	3546.086264	17.053479	-0.054988	3.263564
283.398198	3538.099023	17.058483	-0.055022	3.260125
283.357706	3530.116329	17.063488	-0.055009	3.256674
283.370988	3522.129250	17.068493	-0.055006	3.253219
283.060104	3514.131463	17.073498	-0.054943	3.249743
283.173143	3506.153709	17.078503	-0.054959	3.246290
283.224075	3498.195881	17.083507	-0.054963	3.242838
283.109938	3490.198572	17.088512	-0.054937	3.239359
283.029662	3482.242647	17.093517	-0.054917	3.235896
283.034632	3474.160503	17.098522	-0.054912	3.232378
282.972677	3466.149951	17.103527	-0.054896	3.228884
283.050273	3458.163688	17.108531	-0.054905	3.225402
282.986235	3450.194255	17.113536	-0.054888	3.221919
282.950430	3442.212277	17.118541	-0.054876	3.218427
282.700725	3434.242669	17.123546	-0.054824	3.214928
282.863649	3426.241618	17.128551	-0.054849	3.211429
282.814190	3418.268523	17.133555	-0.054835	3.207929
282.711302	3410.260891	17.138560	-0.054811	3.204408
282.703181	3402.341147	17.143565	-0.054804	3.200926
282.613139	3394.338548	17.148570	-0.054782	3.197400
282.410743	3386.347713	17.153575	-0.054739	3.193871
282.375933	3378.328632	17.158579	-0.054727	3.190332
282.471403	3370.318048	17.163584	-0.054740	3.186798
282.378790	3362.354053	17.168589	-0.054718	3.183274
282.616262	3354.348969	17.173594	-0.054757	3.179741
282.343628	3346.388264	17.178599	-0.054701	3.176202
282.360752	3338.411506	17.183603	-0.054699	3.172664
282.383380	3330.374249	17.188608	-0.054698	3.169096
282.263975	3322.407481	17.193613	-0.054670	3.165549
282.331563	3314.436514	17.198618	-0.054678	3.162005
282.161976	3306.458240	17.203623	-0.054641	3.158442
282.075988	3298.494920	17.208627	-0.054620	3.154886
281.945370	3290.431083	17.213632	-0.054590	3.151280
281.918946	3282.471065	17.218637	-0.054580	3.147720
281.957135	3274.448922	17.223642	-0.054582	3.144130
282.027222	3266.459954	17.228647	-0.054590	3.140554
282.050775	3258.532613	17.233651	-0.054589	3.136998
281.806985	3250.512014	17.238656	-0.054538	3.133385
282.020915	3242.526475	17.243661	-0.054573	3.129804
281.991616	3234.549724	17.248666	-0.054562	3.126212
281.681897	3226.585663	17.253671	-0.054500	3.122609
281.524722	3218.631739	17.258675	-0.054465	3.119013
281.583287	3210.626277	17.263680	-0.054471	3.115399
281.498018	3202.622309	17.268685	-0.054450	3.111775
281.384295	3194.633993	17.273690	-0.054423	3.108153
281.508549	3186.625773	17.278695	-0.054441	3.104528
281.495508	3178.681836	17.283699	-0.054434	3.100923
281.356720	3170.691772	17.288704	-0.054403	3.097286
281.395417	3162.689221	17.293709	-0.054405	3.093647
281.361191	3154.675319	17.298714	-0.054393	3.089996
281.420977	3146.710013	17.303719	-0.054399	3.086366
281.338003	3138.739083	17.308723	-0.054378	3.082723
281.308190	3130.736741	17.313728	-0.054368	3.079065
281.213125	3122.799638	17.318733	-0.054345	3.075428
281.064137	3114.722180	17.323738	-0.054312	3.071720
281.251816	3106.684215	17.328743	-0.054342	3.068042
281.088294	3098.747330	17.333747	-0.054306	3.064389
280.848083	3090.812222	17.338752	-0.054256	3.060729
280.929356	3082.815861	17.343757	-0.054266	3.057052
281.094882	3074.804870	17.348762	-0.054292	3.053367
280.982470	3066.816480	17.353767	-0.054265	3.049676
280.775612	3058.880637	17.358771	-0.054222	3.045999
281.067179	3050.869343	17.363776	-0.054271	3.042307
281.031149	3042.921694	17.368781	-0.054259	3.038624
280.899017	3034.916274	17.373786	-0.054229	3.034906
280.710890	3026.920496	17.378791	-0.054189	3.031184
280.880498	3018.941085	17.383795	-0.054215	3.027483
280.699599	3010.938794	17.388800	-0.054176	3.023750
280.649463	3002.994437	17.393805	-0.054162	3.020045
280.637422	2995.011740	17.398810	-0.054155	3.016320
280.757139	2987.005080	17.403815	-0.054172	3.012586
280.643167	2979.005453	17.408819	-0.054145	3.008838
280.674913	2971.027853	17.413824	-0.054146	3.005104
280.605939	2963.098706	17.418829	-0.054128	3.001382
280.536305	2955.126336	17.423834	-0.054110	2.997636
280.290098	2947.130193	17.428839	-0.054059	2.993865
280.396394	2939.095669	17.433843	-0.054073	2.990088
280.393258	2931.098737	17.438848	-0.054068	2.986319
280.396540	2923.117172	17.443853	-0.054063	2.982553
280.142291	2915.173100	17.448858	-0.054010	2.978787
280.245694	2907.164136	17.453863	-0.054025	2.975004
280.265064	2899.189436	17.458867	-0.054023	2.971227
280.045167	2891.206395	17.463872	-0.053977	2.967430
280.149207	2883.217355	17.468877	-0.053991	2.963642
280.198292	2875.233226	17.473882	-0.053995	2.959848
280.074584	2867.291007	17.478887	-0.053967	2.956060
280.180751	2859.255718	17.483891	-0.053981	2.952235
280.115271	2851.271546	17.488896	-0.053964	2.948421
280.035645	2843.294703	17.493901	-0.053944	2.944604
280.006181	2835.357362	17.498906	-0.053933	2.940804
280.046229	2827.350479	17.503911	-0.053936	2.936969
279.911942	2819.399003	17.508915	-0.053905	2.933147
279.764425	2811.373037	17.513920	-0.053873	2.929283
279.904344	2803.424944	17.518925	-0.053894	2.925467
279.828708	2795.438176	17.523930	-0.053874	2.921615
279.831594	2787.465024	17.528935	-0.053870	2.917770
279.811514	2779.473896	17.533939	-0.053861	2.913909
279.548412	2771.402027	17.538944	-0.053806	2.909991
279.515569	2763.464635	17.543949	-0.053795	2.906146
279.690788	2755.476215	17.548954	-0.053823	2.902281
279.651802	2747.512372	17.553959	-0.053810	2.898412
279.660380	2739.551996	17.558963	-0.053807	2.894542
279.220980	2731.565423	17.563968	-0.053720	2.890630
279.406653	2723.576786	17.568973	-0.053749	2.886745
279.414163	2715.614791	17.573978	-0.053745	2.882858
279.242226	2707.626730	17.578983	-0.053708	2.878944
279.271043	2699.677562	17.583987	-0.053708	2.875054
279.459177	2691.622028	17.588992	-0.053738	2.871116
279.383718	2683.644478	17.593997	-0.053719	2.867196
279.218216	2675.689253	17.599002	-0.053683	2.863277
279.228415	2667.715116	17.604007	-0.053680	2.859352
279.242456	2659.788201	17.609011	-0.053677	2.855446
278.978462	2651.791607	17.614016	-0.053623	2.851485
279.029153	2643.790277	17.619021	-0.053627	2.847533
278.912364	2635.832221	17.624026	-0.053600	2.843587
278.969067	2627.842312	17.629031	-0.053605	2.839631
279.139883	2619.876948	17.634035	-0.053632	2.835687
278.815483	2611.870946	17.639040	-0.053566	2.831689
278.716323	2603.898395	17.644045	-0.053543	2.827716
278.789824	2595.892357	17.649050	-0.053551	2.823730
278.886363	2587.920577	17.654055	-0.053564	2.819756
278.824547	2579.982487	17.659059	-0.053547	2.815785
278.639023	2571.969473	17.664064	-0.053508	2.811764
278.562290	2564.004067	17.669069	-0.053488	2.807767
278.551807	2556.033097	17.674074	-0.053481	2.803765
278.388391	2548.058254	17.679079	-0.053445	2.799746
278.517390	2540.094019	17.684083	-0.053464	2.795745
278.543259	2532.081262	17.689088	-0.053464	2.791707
278.445447	2524.105540	17.694093	-0.053440	2.787674
278.350244	2516.133088	17.699098	-0.053417	2.783638
278.320679	2508.157224	17.704103	-0.053407	2.779598
278.427779	2500.221968	17.709107	-0.053422	2.775580
278.490964	2492.184080	17.714112	-0.053428	2.771502
278.349548	2484.226062	17.719117	-0.053397	2.767447
278.294595	2476.280692	17.724122	-0.053381	2.763397
278.134175	2468.295753	17.729127	-0.053346	2.759315
278.366547	2460.333391	17.734131	-0.053384	2.755261
278.153907	2452.260548	17.739136	-0.053339	2.751119
277.971869	2444.306590	17.744141	-0.053300	2.747033
277.812658	2436.358225	17.749146	-0.053266	2.742945
277.897584	2428.373511	17.754151	-0.053276	2.738847
278.077820	2420.411236	17.759155	-0.053305	2.734760
277.769699	2412.424858	17.764160	-0.053242	2.730625
278.079587	2404.441401	17.769165	-0.053295	2.726523
277.847529	2396.504692	17.774170	-0.053246	2.722406
277.736989	2388.542742	17.779175	-0.053220	2.718276
277.763090	2380.568217	17.784179	-0.053220	2.714143
277.689723	2372.539627	17.789184	-0.053201	2.709969
277.861701	2364.571436	17.794189	-0.053228	2.705835
277.721105	2356.626463	17.799194	-0.053197	2.701687
277.649795	2348.638807	17.804199	-0.053178	2.697515
277.836850	2340.659322	17.809203	-0.053208	2.693358
277.569854	2332.682397	17.814208	-0.053153	2.689166
277.533945	2324.730039	17.819213	-0.053141	2.684995
277.730275	2316.765541	17.824218	-0.053172	2.680827
277.542769	2308.817082	17.829223	-0.053132	2.676635
277.428383	2300.846245	17.834227	-0.053106	2.672430
277.436890	2292.808623	17.839232	-0.053102	2.668191
277.254433	2284.862508	17.844237	-0.053063	2.663981
277.202561	2276.890148	17.849242	-0.053048	2.659760
277.390642	2268.917077	17.854247	-0.053078	2.655546
277.289687	2260.956037	17.859251	-0.053054	2.651314
277.192486	2252.977969	17.864256	-0.053031	2.647065
277.001269	2245.026927	17.869261	-0.052990	2.642819
277.023611	2237.056401	17.874266	-0.052989	2.638569
276.959850	2229.075135	17.879271	-0.052972	2.634301
276.980622	2221.088845	17.884275	-0.052971	2.630028
276.908084	2213.122666	17.889280	-0.052952	2.625754
276.988822	2205.152005	17.894285	-0.052962	2.621480
276.796000	2197.202924	17.899290	-0.052921	2.617192
276.634865	2189.227722	17.904295	-0.052886	2.612886
276.790452	2181.234523	17.909299	-0.052909	2.608584
276.549212	2173.286453	17.914304	-0.052859	2.604272
276.527490	2165.322898	17.919309	-0.052850	2.599960
276.514085	2157.370951	17.924314	-0.052842	2.595647
276.235837	2149.247644	17.929319	-0.052785	2.591216
276.299440	2141.255003	17.934323	-0.052792	2.586872
276.304294	2133.303142	17.939328	-0.052788	2.582539
276.442258	2125.367339	17.944333	-0.052808	2.578217
276.228012	2117.439124	17.949338	-0.052763	2.573867
276.296948	2109.434675	17.954343	-0.052771	2.569487
276.451674	2101.477921	17.959347	-0.052795	2.565132
276.349568	2093.538926	17.964352	-0.052770	2.560762
275.955194	2085.637196	17.969357	-0.052692	2.556384
276.066991	2077.640141	17.974362	-0.052707	2.551982
276.087200	2069.635120	17.979367	-0.052706	2.547561
276.130555	2061.678802	17.984371	-0.052709	2.543161
276.290442	2053.699727	17.989376	-0.052733	2.538749
276.215398	2045.768297	17.994381	-0.052714	2.534339
276.070726	2037.797640	17.999386	-0.052682	2.529895
276.060542	2029.815762	18.004391	-0.052675	2.525446
276.045954	2021.872540	18.009395	-0.052667	2.521010
275.899222	2013.936261	18.014400	-0.052635	2.516562
275.681499	2005.960858	18.019405	-0.052589	2.512078
275.800528	1997.955957	18.024410	-0.052606	2.507594
275.703245	1989.978733	18.029415	-0.052583	2.503101
275.525822	1982.061386	18.034419	-0.052545	2.498629
275.719870	1974.060024	18.039424	-0.052575	2.494128
275.605933	1966.088273	18.044429	-0.052549	2.489613
275.467845	1958.160062	18.049434	-0.052518	2.485113
275.509799	1950.177295	18.054439	-0.052521	2.480587
275.472155	1942.264134	18.059443	-0.052509	2.476087
275.300013	1934.267578	18.064448	-0.052471	2.471521
275.176381	1926.303634	18.069453	-0.052443	2.466968
275.316401	1918.334233	18.074458	-0.052464	2.462424
275.181741	1910.384854	18.079463	-0.052434	2.457862
275.361179	1902.411090	18.084467	-0.052462	2.453301
275.039237	1894.451292	18.089472	-0.052397	2.448702
275.154398	1886.473624	18.094477	-0.052413	2.444117
275.229571	1878.528540	18.099482	-0.052422	2.439539
275.027963	1870.597257	18.104487	-0.052379	2.434940
275.066102	1862.551703	18.109491	-0.052381	2.430284
275.015646	1854.579200	18.114496	-0.052367	2.425654
274.906916	1846.653794	18.119501	-0.052341	2.421039
274.918752	1838.705903	18.124506	-0.052338	2.416411
274.803572	1830.729673	18.129511	-0.052312	2.411747
274.735257	1822.784581	18.134515	-0.052294	2.407097
274.645395	1814.827930	18.139520	-0.052272	2.402429
274.724895	1806.881498	18.144525	-0.052282	2.397771
274.684837	1798.924501	18.149530	-0.052269	2.393088
274.438592	1790.961947	18.154535	-0.052218	2.388377
274.723518	1782.984328	18.159539	-0.052266	2.383690
274.800381	1775.012919	18.164544	-0.052275	2.378980
274.645193	1767.082587	18.169549	-0.052241	2.374267
274.439877	1759.132819	18.174554	-0.052197	2.369529
274.627998	1751.125950	18.179559	-0.052227	2.364779
274.619984	1743.220310	18.184563	-0.052221	2.360064
274.310911	1735.303759	18.189568	-0.052158	2.355309
274.331120	1727.283873	18.194573	-0.052157	2.350509
274.241193	1719.338399	18.199578	-0.052135	2.345735
274.109008	1711.392830	18.204583	-0.052105	2.340947
274.240464	1703.452656	18.209587	-0.052124	2.336175
274.256517	1695.459822	18.214592	-0.052122	2.331352
273.976484	1687.532318	18.219597	-0.052065	2.326533
273.863260	1679.596359	18.224602	-0.052038	2.321713
273.938404	1671.629666	18.229607	-0.052047	2.316881
274.028841	1663.664891	18.234611	-0.052059	2.312040
273.905485	1655.704318	18.239616	-0.052031	2.307174
273.647117	1647.791873	18.244621	-0.051977	2.302316
273.903802	1639.806751	18.249626	-0.052020	2.297446
273.686632	1631.867948	18.254631	-0.051974	2.292555
273.733693	1623.908329	18.259635	-0.051978	2.287662
273.767977	1615.953797	18.264640	-0.051979	2.282761
273.555821	1608.034681	18.269645	-0.051935	2.277851
273.452189	1600.067403	18.274650	-0.051910	2.272909
273.449086	1592.038761	18.279655	-0.051904	2.267927
273.726180	1584.075667	18.284659	-0.051951	2.262999
273.398184	1576.176427	18.289664	-0.051885	2.258047
273.479937	1568.215303	18.294669	-0.051895	2.253082
273.553861	1560.252820	18.299674	-0.051903	2.248104
273.355799	1552.326432	18.304679	-0.051861	2.243114
273.211904	1544.417933	18.309683	-0.051829	2.238129
273.111323	1536.469868	18.314688	-0.051805	2.233111
273.246190	1528.483315	18.319693	-0.051825	2.228079
273.287632	1520.542323	18.324698	-0.051828	2.223056
273.178049	1512.598653	18.329703	-0.051802	2.218006
273.156664	1504.673490	18.334707	-0.051793	2.212965
272.855673	1496.745799	18.339712	-0.051732	2.207885
272.881677	1488.806824	18.344717	-0.051732	2.202815
272.941501	1480.868411	18.349722	-0.051738	2.197738
272.658304	1472.924117	18.354727	-0.051680	2.192613
272.667395	1464.959404	18.359731	-0.051676	2.187491
272.812116	1456.979358	18.364736	-0.051698	2.182358
272.826291	1449.036728	18.369741	-0.051695	2.177226
272.663807	1441.124902	18.374746	-0.051660	2.172085
272.507492	1433.172446	18.379751	-0.051626	2.166906
272.737853	1425.215389	18.384755	-0.051664	2.161748
272.619357	1417.295842	18.389760	-0.051636	2.156569
272.278149	1409.376427	18.394765	-0.051568	2.151358
272.583403	1401.391815	18.399770	-0.051619	2.146151
272.474262	1393.464341	18.404775	-0.051594	2.140930
272.354204	1385.564457	18.409779	-0.051566	2.135714
272.242454	1377.611464	18.414784	-0.051540	2.130450
272.516474	1369.628366	18.419789	-0.051586	2.125190
272.490050	1361.728270	18.424794	-0.051576	2.119944
272.363508	1353.802187	18.429799	-0.051547	2.114658
272.100089	1345.828588	18.434803	-0.051493	2.109313
272.047900	1337.886797	18.439808	-0.051478	2.103997
271.981181	1329.972317	18.444813	-0.051461	2.098684
271.999524	1322.036356	18.449818	-0.051459	2.093351
271.822275	1314.099233	18.454823	-0.051421	2.087985
271.717778	1306.184514	18.459827	-0.051396	2.082627
271.876399	1298.237661	18.464832	-0.051421	2.077259
271.913401	1290.285083	18.469837	-0.051422	2.071862
271.907762	1282.352302	18.474842	-0.051416	2.066460
271.534928	1274.463982	18.479847	-0.051342	2.061037
271.873860	1266.498251	18.484851	-0.051400	2.055619
271.633378	1258.580650	18.489856	-0.051350	2.050160
271.554406	1250.663777	18.494861	-0.051330	2.044704
271.624049	1242.727043	18.499866	-0.051338	2.039235
271.465802	1234.817322	18.504871	-0.051303	2.033747
271.541444	1226.850343	18.509875	-0.051312	2.028227
271.238431	1218.961693	18.514880	-0.051250	2.022709
271.216996	1211.043156	18.519885	-0.051241	2.017183
271.260398	1203.103517	18.524890	-0.051244	2.011634
271.258329	1195.146004	18.529895	-0.051239	2.006053
271.236793	1187.248960	18.534899	-0.051229	2.000496
271.142268	1179.344675	18.539904	-0.051207	1.994911
270.993027	1171.406790	18.544909	-0.051174	1.989281
271.136615	1163.458670	18.549914	-0.051195	1.983659
271.093870	1155.550838	18.554919	-0.051182	1.978029
271.021469	1147.642852	18.559923	-0.051164	1.972381
271.154982	1139.691281	18.564928	-0.051183	1.966706
270.914764	1131.803203	18.569933	-0.051133	1.961021
271.245420	1123.858966	18.574938	-0.051190	1.955341
270.917194	1115.928090	18.579943	-0.051124	1.949582
270.844075	1108.023291	18.584947	-0.051105	1.943852
270.604667	1100.135475	18.589952	-0.051055	1.938100
270.415866	1092.235369	18.594957	-0.051015	1.932328
270.499789	1084.290365	18.599962	-0.051025	1.926535
270.506403	1076.359753	18.604967	-0.051021	1.920726
270.562048	1068.455020	18.609971	-0.051027	1.914925
270.377770	1060.542353	18.614976	-0.050987	1.909073
270.181324	1052.648323	18.619981	-0.050945	1.903216
270.138440	1044.750183	18.624986	-0.050932	1.897355
270.185441	1036.807692	18.629991	-0.050936	1.891452
270.508187	1028.855514	18.634995	-0.050991	1.885556
270.337308	1020.992008	18.640000	-0.050954	1.879651
270.270142	1013.092885	18.645005	-0.050936	1.873712
270.334678	1005.155276	18.650010	-0.050943	1.867741
270.141365	997.271839	18.655015	-0.050902	1.861762
269.987800	989.394208	18.660019	-0.050868	1.855772
270.039492	981.458615	18.665024	-0.050873	1.849743
269.937529	973.568701	18.670029	-0.050849	1.843711
269.664511	965.717897	18.675034	-0.050793	1.837669
269.589984	957.796043	18.680039	-0.050774	1.831576
269.728471	949.867986	18.685043	-0.050794	1.825482
269.665385	941.985815	18.690048	-0.050777	1.819381
269.484579	934.099257	18.695053	-0.050739	1.813240
269.451615	926.196269	18.700058	-0.050727	1.807085
269.430135	918.298271	18.705063	-0.050718	1.800913
269.389945	910.423860	18.710067	-0.050706	1.794736
269.226216	902.486143	18.715072	-0.050670	1.788473
269.439565	894.554506	18.720077	-0.050705	1.782239
269.476286	886.674690	18.725082	-0.050706	1.776002
269.154314	878.813416	18.730087	-0.050641	1.769714
269.302127	870.907899	18.735091	-0.050664	1.763427
269.248735	863.040572	18.740096	-0.050649	1.757122
269.232120	855.144728	18.745101	-0.050640	1.750777
269.224253	847.264707	18.750106	-0.050634	1.744422
269.119292	839.400262	18.755111	-0.050609	1.738044
269.107786	831.519386	18.760115	-0.050602	1.731641
269.085587	823.624576	18.765120	-0.050593	1.725202
268.803711	815.797172	18.770125	-0.050535	1.718760
268.787547	807.914646	18.775130	-0.050527	1.712283
268.591039	800.030802	18.780135	-0.050485	1.705757
268.573937	792.161764	18.785139	-0.050477	1.699242
268.518966	784.281409	18.790144	-0.050461	1.692687
268.349564	776.407648	18.795149	-0.050425	1.686097
268.633068	768.514467	18.800154	-0.050472	1.679525
268.644777	760.632658	18.805159	-0.050470	1.672900
268.601295	752.755688	18.810163	-0.050456	1.666246
268.320078	744.941875	18.815168	-0.050399	1.659586
268.297406	737.077505	18.820173	-0.050390	1.652892
268.480264	729.174653	18.825178	-0.050418	1.646166
268.164875	721.370956	18.830183	-0.050355	1.639428
268.328401	713.474847	18.835187	-0.050380	1.632650
268.210932	705.576429	18.840192	-0.050353	1.625802
267.955381	697.765005	18.845197	-0.050300	1.618981
267.902996	689.916823	18.850202	-0.050285	1.612128
267.872321	682.040903	18.855207	-0.050275	1.605224
267.950402	674.208270	18.860211	-0.050284	1.598344
267.824587	666.358787	18.865216	-0.050256	1.591391
267.806660	658.501209	18.870221	-0.050247	1.584415
267.858729	650.667596	18.875226	-0.050252	1.577440
267.536398	642.841243	18.880231	-0.050187	1.570385
267.806899	634.965465	18.885235	-0.050232	1.563341
267.771005	627.143679	18.890240	-0.050220	1.556269
267.623731	619.302513	18.895245	-0.050188	1.549131
267.607783	611.478330	18.900250	-0.050180	1.541995
267.549217	603.637035	18.905255	-0.050164	1.534803
267.401466	595.827338	18.910259	-0.050131	1.527593
267.064259	588.052239	18.915264	-0.050063	1.520353
267.196836	580.196060	18.920269	-0.050083	1.513073
267.307040	572.339728	18.925274	-0.050098	1.505755
267.012841	564.567142	18.930279	-0.050038	1.498417
267.206867	556.707165	18.935283	-0.050069	1.491037
266.971282	548.924856	18.940288	-0.050020	1.483626
266.875004	541.132137	18.945293	-0.049997	1.476190
266.638127	533.307241	18.950298	-0.049948	1.468664
266.674781	525.469149	18.955303	-0.049950	1.461129
266.775126	517.660063	18.960307	-0.049964	1.453594
266.618160	509.863597	18.965312	-0.049929	1.445990
266.639711	502.066545	18.970317	-0.049928	1.438374
266.924996	494.225783	18.975322	-0.049976	1.430717
266.775779	486.453198	18.980327	-0.049943	1.423016
266.543242	478.713338	18.985331	-0.049895	1.415292
266.641237	470.902113	18.990336	-0.049908	1.407508
266.595701	463.133137	18.995341	-0.049895	1.399700
266.616693	455.353399	19.000346	-0.049894	1.391849
266.443376	447.580392	19.005351	-0.049856	1.383926
266.321785	439.833942	19.010355	-0.049829	1.375994
266.166747	432.077755	19.015360	-0.049795	1.368001
265.947325	424.340800	19.020365	-0.049749	1.359969
265.983797	416.569734	19.025370	-0.049751	1.351898
266.024596	408.782245	19.030375	-0.049753	1.343762
265.778536	401.073779	19.035379	-0.049702	1.335610
265.858585	393.292411	19.040384	-0.049712	1.327387
265.840629	385.555326	19.045389	-0.049704	1.319144
265.701609	377.758515	19.050394	-0.049673	1.310762
265.403965	370.004790	19.055399	-0.049612	1.302344
265.462201	362.273080	19.060403	-0.049618	1.293961
265.274514	354.563497	19.065408	-0.049578	1.285502
265.363650	346.843407	19.070413	-0.049590	1.277026
265.397094	339.113831	19.075418	-0.049591	1.268473
265.259704	331.420288	19.080423	-0.049560	1.259870
265.309230	323.714527	19.085427	-0.049565	1.251229
265.421247	315.999062	19.090432	-0.049580	1.242530
265.362620	308.317464	19.095437	-0.049565	1.233774
265.018645	300.672007	19.100442	-0.049495	1.224942
264.846369	293.005398	19.105447	-0.049458	1.216055
265.025344	285.291263	19.110451	-0.049487	1.207117
264.753827	277.670221	19.115456	-0.049431	1.198131
264.835715	269.977352	19.120461	-0.049441	1.189064
264.710614	262.343208	19.125466	-0.049413	1.179955
264.540047	254.705019	19.130471	-0.049377	1.170761
264.511299	247.064431	19.135475	-0.049366	1.161520
264.496746	239.417955	19.140480	-0.049359	1.152201
264.459183	231.751045	19.145485	-0.049347	1.142776
264.428167	224.144995	19.150490	-0.049336	1.133350
264.365113	216.523179	19.155495	-0.049319	1.123818
264.288311	208.944407	19.160499	-0.049300	1.114256
263.988866	201.383394	19.165504	-0.049239	1.104584
263.996545	193.784857	19.170509	-0.049236	1.094847
264.131358	186.180482	19.175514	-0.049256	1.085044
263.980526	178.637348	19.180519	-0.049223	1.075166
263.772928	171.092432	19.185523	-0.049179	1.065182
263.778507	163.539796	19.190528	-0.049175	1.055142
263.585773	156.022416	19.195533	-0.049135	1.045007
263.538884	148.505097	19.200538	-0.049121	1.034807
263.361671	140.991583	19.205543	-0.049083	1.024480
263.426581	133.478852	19.210547	-0.049090	1.014107
263.430223	125.978014	19.215552	-0.049086	1.003628
263.138458	118.535669	19.220557	-0.049027	0.993049
263.163516	111.031637	19.225562	-0.049027	0.982346
262.967652	103.600055	19.230567	-0.048986	0.971575
262.919927	96.164298	19.235571	-0.048972	0.960715
262.884466	88.735368	19.240576	-0.048960	0.949744
262.882552	81.309991	19.245581	-0.048955	0.938658
262.645420	73.962458	19.250586	-0.048906	0.927496
262.666804	66.579654	19.255591	-0.048905	0.916213
262.715692	59.422911	19.260595	-0.048910	0.905150