Fri Mar 12 12:24:31 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.385681	0.193209	0.000000	0.000048	0.720865
0.491589	0.179812	0.005005	0.000028	0.720875
0.449600	0.185493	0.010010	0.000036	0.720872
0.471418	0.058188	0.015014	0.000032	0.720629
0.476809	0.012099	0.020019	0.000031	0.720540
0.507408	0.001208	0.025024	0.000025	0.720529
0.334130	0.035781	0.030029	0.000058	0.720537
0.443571	0.016003	0.035034	0.000037	0.720536
0.354705	0.028924	0.040038	0.000054	0.720530
0.353548	0.033083	0.045043	0.000054	0.720538
0.321401	0.035506	0.050048	0.000060	0.720531
0.364799	0.031652	0.055053	0.000052	0.720539
0.433328	0.016781	0.060058	0.000039	0.720534
0.378259	0.025507	0.065062	0.000050	0.720531
0.509196	0.006618	0.070067	0.000025	0.720540
0.632003	-0.020099	0.075072	0.000003	0.720530
0.613794	-0.012268	0.080077	0.000006	0.720539
0.692710	-0.119644	0.085082	-0.000009	0.720356
0.636585	-0.179727	0.090086	0.000002	0.720218
0.514104	-0.153408	0.095091	0.000025	0.720226
0.413188	-0.140916	0.100096	0.000044	0.720215
0.484546	-0.149315	0.105101	0.000030	0.720224
0.387427	-0.130882	0.110106	0.000048	0.720226
0.381883	-0.173690	0.115110	0.000049	0.720140
0.502430	-0.316235	0.120115	0.000027	0.719901
0.474157	-0.316558	0.125120	0.000032	0.719891
0.490323	-0.315012	0.130125	0.000029	0.719899
0.292151	-0.279889	0.135130	0.000066	0.719899
0.402449	-0.332971	0.140134	0.000046	0.719833
0.610637	-0.484421	0.145139	0.000007	0.719607
0.373782	-0.447793	0.150144	0.000051	0.719596
0.432320	-0.454705	0.155149	0.000041	0.719603
0.487515	-0.473573	0.160154	0.000030	0.719585
0.376922	-0.614872	0.165158	0.000051	0.719268
0.531761	-0.638937	0.170163	0.000022	0.719275
0.443075	-0.627348	0.175168	0.000039	0.719266
0.522810	-0.697394	0.180173	0.000024	0.719156
0.396985	-0.773586	0.185178	0.000047	0.718962
0.544793	-0.802493	0.190182	0.000020	0.718956
0.336836	-0.767326	0.195187	0.000059	0.718953
0.239917	-0.909968	0.200192	0.000077	0.718637
0.347621	-0.924496	0.205197	0.000057	0.718646
0.521806	-0.956756	0.210202	0.000025	0.718644
0.286344	-1.048963	0.215206	0.000068	0.718379
0.389028	-1.077737	0.220211	0.000049	0.718358
0.299198	-1.065740	0.225216	0.000066	0.718350
0.280877	-1.224894	0.230221	0.000070	0.718029
0.218741	-1.220000	0.235226	0.000081	0.718017
0.277573	-1.266675	0.240230	0.000070	0.717945
0.202882	-1.373288	0.245235	0.000084	0.717708
0.182754	-1.373939	0.250240	0.000088	0.717700
0.317824	-1.492885	0.255245	0.000063	0.717512
0.288758	-1.552969	0.260250	0.000069	0.717383
0.147897	-1.546322	0.265254	0.000095	0.717347
0.249290	-1.692840	0.270259	0.000076	0.717093
0.223751	-1.693904	0.275264	0.000081	0.717081
0.039258	-1.781247	0.280269	0.000115	0.716843
-0.097374	-1.802353	0.285274	0.000141	0.716753
-0.225891	-1.835543	0.290278	0.000165	0.716642
0.049039	-1.980919	0.295283	0.000114	0.716452
-0.125420	-1.965502	0.300288	0.000146	0.716420
0.033904	-2.139038	0.305293	0.000117	0.716133
0.040606	-2.141149	0.310298	0.000115	0.716131
-0.111044	-2.233275	0.315302	0.000144	0.715895
-0.312698	-2.202602	0.320307	0.000181	0.715884
-1.191022	-2.183307	0.325312	0.000345	0.715613
-3.220201	-1.855613	0.330317	0.000723	0.715546
-2.734783	-1.940168	0.335322	0.000632	0.715549
-3.024132	-2.026626	0.340326	0.000686	0.715276
-4.196814	-1.837717	0.345331	0.000905	0.715236
-3.787343	-1.916379	0.350336	0.000828	0.715224
-3.082865	-2.109602	0.355341	0.000697	0.715090
-4.799809	-1.894958	0.360346	0.001017	0.714909
-4.588294	-1.935718	0.365350	0.000978	0.714903
-4.111885	-2.015725	0.370355	0.000889	0.714912
-5.020816	-1.982039	0.375360	0.001058	0.714658
-5.757972	-1.875096	0.380365	0.001195	0.714609
-5.494566	-1.922977	0.385370	0.001146	0.714607
-5.406089	-1.941306	0.390374	0.001130	0.714602
-5.641028	-1.986290	0.395379	0.001174	0.714430
-6.757544	-1.866844	0.400384	0.001382	0.714272
-6.381122	-1.930617	0.405389	0.001312	0.714278
-6.491352	-1.910478	0.410394	0.001332	0.714279
-6.875939	-1.844329	0.415398	0.001404	0.714274
-6.370938	-2.028955	0.420403	0.001310	0.714086
-7.393332	-1.906989	0.425408	0.001500	0.713967
-7.436286	-1.897893	0.430413	0.001508	0.713970
-7.220547	-1.936655	0.435418	0.001468	0.713969
-7.469912	-1.895616	0.440422	0.001515	0.713962
-7.719789	-1.922384	0.445427	0.001561	0.713820
-8.652343	-1.844034	0.450432	0.001735	0.713646
-7.994244	-1.958234	0.455437	0.001612	0.713652
-7.988982	-1.959653	0.460442	0.001611	0.713651
-8.720499	-1.831294	0.465446	0.001748	0.713647
-7.729125	-2.003970	0.470451	0.001563	0.713655
-8.361937	-2.016639	0.475456	0.001681	0.713405
-9.447357	-1.845039	0.480461	0.001883	0.713362
-8.878987	-1.944394	0.485466	0.001777	0.713365
-8.629964	-1.994070	0.490470	0.001731	0.713355
-9.170325	-1.893645	0.495475	0.001832	0.713363
-9.271184	-1.890125	0.500480	0.001850	0.713334
-9.687598	-1.971763	0.505485	0.001928	0.713024
-9.781533	-1.955468	0.510490	0.001945	0.713023
-10.307648	-1.862758	0.515494	0.002043	0.713021
-9.751662	-1.955792	0.520499	0.001940	0.713033
-10.145469	-1.891754	0.525504	0.002013	0.713021
-10.514502	-1.825110	0.530509	0.002082	0.713022
-10.080855	-2.004423	0.535514	0.002001	0.712819
-11.017237	-1.895302	0.540518	0.002176	0.712704
-10.736937	-1.939415	0.545523	0.002124	0.712716
-10.977512	-1.902009	0.550528	0.002168	0.712705
-10.898952	-1.913548	0.555533	0.002154	0.712710
-10.679019	-1.951923	0.560538	0.002113	0.712711
-11.312502	-1.864541	0.565542	0.002231	0.712661
-11.633314	-1.942836	0.570547	0.002291	0.712391
-11.528344	-1.965116	0.575552	0.002271	0.712384
-11.967529	-1.886597	0.580557	0.002353	0.712384
-12.023856	-1.877003	0.585562	0.002363	0.712383
-11.868644	-1.907686	0.590566	0.002335	0.712377
-11.876663	-1.900194	0.595571	0.002336	0.712389
-11.976511	-1.922614	0.600576	0.002355	0.712309
-12.481865	-1.945632	0.605581	0.002449	0.712084
-12.248664	-1.983710	0.610586	0.002405	0.712090
-12.850701	-1.880832	0.615590	0.002518	0.712082
-12.586004	-1.923269	0.620595	0.002468	0.712091
-12.411034	-1.957198	0.625600	0.002436	0.712085
-12.807355	-1.885258	0.630605	0.002510	0.712088
-12.868175	-1.988623	0.635610	0.002521	0.711860
-13.766208	-1.882798	0.640614	0.002688	0.711752
-13.597110	-1.907224	0.645619	0.002657	0.711764
-13.738902	-1.887293	0.650624	0.002683	0.711753
-13.861069	-1.863538	0.655629	0.002706	0.711757
-13.272162	-1.966607	0.660634	0.002596	0.711760
-13.680620	-1.897240	0.665638	0.002672	0.711754
-13.992445	-1.929130	0.670643	0.002730	0.711579
-14.560523	-1.894323	0.675648	0.002836	0.711447
-14.277436	-1.944191	0.680653	0.002784	0.711448
-14.430179	-1.914870	0.685658	0.002812	0.711452
-14.746333	-1.862692	0.690662	0.002871	0.711443
-14.118601	-1.969199	0.695667	0.002754	0.711454
-14.470467	-1.909131	0.700672	0.002820	0.711449
-14.679890	-1.982192	0.705677	0.002859	0.711228
-15.450314	-1.891109	0.710682	0.003002	0.711136
-15.573884	-1.873480	0.715686	0.003025	0.711127
-15.101748	-1.952617	0.720691	0.002937	0.711137
-15.325157	-1.915164	0.725696	0.002979	0.711133
-15.450932	-1.892605	0.730701	0.003002	0.711133
-15.318684	-1.914734	0.735706	0.002978	0.711136
-15.494256	-1.977979	0.740710	0.003011	0.710947
-15.979428	-1.929496	0.745715	0.003101	0.710871
-16.259529	-1.883033	0.750720	0.003153	0.710864
-16.276829	-1.877615	0.755725	0.003156	0.710869
-15.901140	-1.944143	0.760730	0.003086	0.710869
-16.204193	-1.894411	0.765734	0.003143	0.710861
-16.299245	-1.873221	0.770739	0.003161	0.710869
-16.424217	-2.007898	0.775744	0.003184	0.710556
-16.938346	-1.930161	0.780749	0.003280	0.710528
-17.132734	-1.893654	0.785754	0.003316	0.710532
-17.179996	-1.888720	0.790758	0.003325	0.710525
-16.793838	-1.953560	0.795763	0.003253	0.710533
-16.938225	-1.931435	0.800768	0.003280	0.710525
-17.006882	-1.948790	0.805773	0.003293	0.710466
-17.711663	-1.948450	0.810778	0.003424	0.710216
-17.873542	-1.923283	0.815782	0.003454	0.710208
-17.997351	-1.897987	0.820787	0.003477	0.710215
-17.703053	-1.952866	0.825792	0.003422	0.710210
-17.800190	-1.934941	0.830797	0.003440	0.710211
-17.966282	-1.902618	0.835802	0.003471	0.710216
-17.853300	-1.980409	0.840806	0.003450	0.710101
-18.461679	-1.975434	0.845811	0.003564	0.709894
-18.874607	-1.905915	0.850816	0.003641	0.709886
-19.062932	-1.871777	0.855821	0.003676	0.709887
-18.559279	-1.960414	0.860826	0.003582	0.709889
-18.642165	-1.948776	0.865830	0.003597	0.709883
-18.981998	-1.883577	0.870835	0.003661	0.709892
-18.856540	-1.957671	0.875840	0.003637	0.709789
-19.530233	-1.936907	0.880845	0.003763	0.709590
-19.421410	-1.954868	0.885850	0.003743	0.709593
-19.887740	-1.875321	0.890854	0.003829	0.709586
-19.576924	-1.924519	0.895859	0.003772	0.709598
-19.619616	-1.921019	0.900864	0.003780	0.709590
-19.724400	-1.901925	0.905869	0.003799	0.709591
-19.537130	-1.999459	0.910874	0.003764	0.709462
-20.910852	-1.857395	0.915878	0.004020	0.709257
-20.759205	-1.879869	0.920883	0.003992	0.709266
-20.758739	-1.883824	0.925888	0.003992	0.709258
-20.471881	-1.934997	0.930893	0.003938	0.709258
-20.498295	-1.928155	0.935898	0.003943	0.709262
-20.955412	-1.850753	0.940902	0.004029	0.709254
-20.509242	-1.925366	0.945907	0.003946	0.709263
-21.017992	-1.991349	0.950912	0.004040	0.708950
-21.623696	-1.881848	0.955917	0.004153	0.708953
-21.533479	-1.896729	0.960922	0.004136	0.708955
-21.403701	-1.924196	0.965926	0.004112	0.708947
-21.844175	-1.841103	0.970931	0.004194	0.708956
-21.778227	-1.855050	0.975936	0.004182	0.708951
-21.605344	-1.886691	0.980941	0.004150	0.708950
-21.730833	-1.958045	0.985946	0.004173	0.708762
-22.886621	-1.817532	0.990950	0.004388	0.708631
-22.143456	-1.943879	0.995955	0.004250	0.708643
-22.210380	-1.937845	1.000960	0.004263	0.708631
-22.682558	-1.852842	1.005965	0.004351	0.708633
-22.246858	-1.927468	1.010970	0.004269	0.708639
-22.408956	-1.903185	1.015974	0.004300	0.708629
-22.627490	-1.931887	1.020979	0.004340	0.708494
-23.538927	-1.844361	1.025984	0.004510	0.708344
-23.305606	-1.886190	1.030989	0.004467	0.708343
-23.146708	-1.911756	1.035994	0.004437	0.708348
-23.678661	-1.821979	1.040998	0.004536	0.708338
-23.232124	-1.896436	1.046003	0.004453	0.708349
-23.385576	-1.872406	1.051008	0.004482	0.708342
-23.641622	-1.836830	1.056013	0.004529	0.708322
-23.698183	-1.981121	1.061018	0.004540	0.708012
-23.962925	-1.940329	1.066022	0.004589	0.707999
-24.363161	-1.863201	1.071027	0.004664	0.708011
-24.211138	-1.893150	1.076032	0.004636	0.708005
-24.254088	-1.885154	1.081037	0.004644	0.708006
-23.975911	-1.933500	1.086042	0.004592	0.708008
-24.225542	-1.927713	1.091046	0.004638	0.707930
-24.863486	-1.929999	1.096051	0.004757	0.707698
-24.532264	-1.991304	1.101056	0.004696	0.707693
-25.160955	-1.879139	1.106061	0.004813	0.707693
-25.146651	-1.876951	1.111066	0.004810	0.707703
-24.971388	-1.914855	1.116070	0.004777	0.707689
-24.986228	-1.907589	1.121075	0.004780	0.707699
-25.154576	-1.950315	1.126080	0.004812	0.707553
-26.068174	-1.878236	1.131085	0.004982	0.707370
-25.493530	-1.978068	1.136090	0.004875	0.707376
-26.012574	-1.890967	1.141094	0.004971	0.707365
-25.964002	-1.895629	1.146099	0.004962	0.707373
-25.680970	-1.947333	1.151104	0.004910	0.707370
-26.168387	-1.860113	1.156109	0.005000	0.707371
-26.007425	-1.955201	1.161114	0.004971	0.707237
-26.782367	-1.900367	1.166118	0.005115	0.707070
-26.532258	-1.937610	1.171123	0.005068	0.707085
-26.982110	-1.860506	1.176128	0.005152	0.707078
-26.816748	-1.891703	1.181133	0.005121	0.707075
-26.487408	-1.947035	1.186138	0.005060	0.707082
-26.925809	-1.873488	1.191142	0.005142	0.707072
-26.876955	-1.968971	1.196147	0.005133	0.706898
-27.894415	-1.862507	1.201152	0.005322	0.706748
-27.686386	-1.900026	1.206157	0.005283	0.706747
-27.868493	-1.863456	1.211162	0.005317	0.706755
-27.889190	-1.864285	1.216166	0.005321	0.706746
-27.688463	-1.897316	1.221171	0.005284	0.706751
-27.576840	-1.921226	1.226176	0.005263	0.706743
-27.961280	-1.880064	1.231181	0.005335	0.706688
-28.304121	-1.940751	1.236186	0.005399	0.706443
-28.681055	-1.877105	1.241190	0.005469	0.706436
-28.700231	-1.868919	1.246195	0.005472	0.706446
-28.356100	-1.933225	1.251200	0.005408	0.706440
-28.493819	-1.909501	1.256205	0.005434	0.706438
-28.549595	-1.897083	1.261210	0.005445	0.706443
-28.373524	-1.973416	1.266214	0.005412	0.706352
-29.335360	-1.915043	1.271219	0.005591	0.706125
-29.359077	-1.913582	1.276224	0.005595	0.706119
-29.391422	-1.907088	1.281229	0.005601	0.706121
-29.060627	-1.962494	1.286234	0.005540	0.706128
-29.458382	-1.897269	1.291238	0.005614	0.706117
-29.867613	-1.821262	1.296243	0.005690	0.706123
-29.467738	-1.934286	1.301248	0.005616	0.706039
-30.345056	-1.869152	1.306253	0.005779	0.705855
-30.070163	-1.914091	1.311258	0.005728	0.705863
-30.333998	-1.873162	1.316262	0.005777	0.705851
-30.100285	-1.909789	1.321267	0.005734	0.705861
-30.049655	-1.920377	1.326272	0.005724	0.705858
-30.390404	-1.860382	1.331277	0.005788	0.705856
-30.077486	-2.011240	1.336282	0.005730	0.705665
-31.616229	-1.812704	1.341286	0.006016	0.705512
-31.152049	-1.890537	1.346291	0.005930	0.705522
-30.727944	-1.968168	1.351296	0.005851	0.705518
-31.375550	-1.852963	1.356301	0.005971	0.705517
-31.084767	-1.901591	1.361306	0.005917	0.705524
-31.082744	-1.906927	1.366310	0.005917	0.705514
-31.237326	-1.983975	1.371315	0.005946	0.705303
-32.331032	-1.840150	1.376320	0.006149	0.705200
-32.166202	-1.869157	1.381325	0.006119	0.705201
-31.718175	-1.943649	1.386330	0.006035	0.705212
-32.168947	-1.868572	1.391334	0.006119	0.705201
-32.225091	-1.855898	1.396339	0.006130	0.705206
-32.173807	-1.867997	1.401344	0.006120	0.705200
-32.320525	-1.909885	1.406349	0.006148	0.705063
-33.349063	-1.815712	1.411354	0.006339	0.704884
-32.971422	-1.885410	1.416358	0.006269	0.704879
-33.255021	-1.831258	1.421363	0.006322	0.704886
-33.315959	-1.823465	1.426368	0.006333	0.704880
-33.126671	-1.859236	1.431373	0.006298	0.704876
-33.035367	-1.872035	1.436378	0.006281	0.704882
-33.299738	-1.828867	1.441382	0.006330	0.704874
-33.264341	-1.928642	1.446387	0.006324	0.704686
-33.908952	-1.866375	1.451392	0.006444	0.704580
-33.879998	-1.872283	1.456397	0.006438	0.704578
-33.756140	-1.890501	1.461402	0.006415	0.704586
-34.219713	-1.812630	1.466406	0.006501	0.704576
-33.801195	-1.882760	1.471411	0.006424	0.704585
-33.885374	-1.869312	1.476416	0.006439	0.704582
-34.359037	-1.884835	1.481421	0.006528	0.704381
-34.777512	-1.870950	1.486426	0.006605	0.704258
-34.563542	-1.913288	1.491430	0.006566	0.704250
-34.756951	-1.875642	1.496435	0.006602	0.704256
-34.795522	-1.868775	1.501440	0.006609	0.704256
-34.747128	-1.878923	1.506445	0.006600	0.704253
-34.610895	-1.898614	1.511450	0.006575	0.704262
-35.075084	-1.931259	1.516454	0.006661	0.704029
-35.607687	-1.873891	1.521459	0.006760	0.703953
-35.448739	-1.902355	1.526464	0.006731	0.703953
-35.687693	-1.861349	1.531469	0.006775	0.703950
-35.517514	-1.888836	1.536474	0.006744	0.703956
-35.570257	-1.884164	1.541478	0.006753	0.703946
-35.581313	-1.880074	1.546483	0.006756	0.703950
-36.050920	-1.941213	1.551488	0.006843	0.703658
-36.413032	-1.889928	1.556493	0.006910	0.703631
-36.635475	-1.846914	1.561498	0.006952	0.703638
-36.659930	-1.845116	1.566502	0.006956	0.703632
-36.425587	-1.884819	1.571507	0.006913	0.703637
-36.645015	-1.847950	1.576512	0.006954	0.703632
-36.925161	-1.800101	1.581517	0.007006	0.703628
-36.439612	-1.979034	1.586522	0.006916	0.703441
-37.306819	-1.876277	1.591526	0.007077	0.703337
-37.279189	-1.878120	1.596531	0.007072	0.703343
-37.307269	-1.875327	1.601536	0.007077	0.703338
-37.414434	-1.857390	1.606541	0.007097	0.703336
-37.295484	-1.874820	1.611546	0.007075	0.703343
-37.440346	-1.852790	1.616550	0.007102	0.703336
-37.885304	-1.930514	1.621555	0.007185	0.703018
-38.049434	-1.908486	1.626560	0.007216	0.703004
-38.692290	-1.794842	1.631565	0.007335	0.703002
-38.221771	-1.875151	1.636570	0.007248	0.703009
-38.001022	-1.919583	1.641574	0.007207	0.702999
-38.318710	-1.860321	1.646579	0.007266	0.703004
-38.286258	-1.866388	1.651584	0.007260	0.703003
-38.882271	-1.908833	1.656589	0.007371	0.702703
-39.161936	-1.862532	1.661594	0.007423	0.702695
-39.507587	-1.806434	1.666598	0.007487	0.702684
-38.949681	-1.902367	1.671603	0.007383	0.702691
-39.117464	-1.871611	1.676608	0.007415	0.702693
-39.547523	-1.796601	1.681613	0.007495	0.702689
-39.020739	-1.887448	1.686618	0.007397	0.702696
-39.257193	-1.960691	1.691622	0.007441	0.702462
-40.282999	-1.823083	1.696627	0.007632	0.702371
-39.996257	-1.876653	1.701632	0.007579	0.702366
-39.966790	-1.884079	1.706637	0.007573	0.702361
-40.105350	-1.854750	1.711642	0.007599	0.702371
-40.175032	-1.845964	1.716646	0.007612	0.702363
-39.909504	-1.891968	1.721651	0.007562	0.702366
-39.951137	-1.987002	1.726656	0.007570	0.702159
-41.024822	-1.843147	1.731661	0.007770	0.702062
-40.467338	-1.936465	1.736666	0.007666	0.702075
-40.596221	-1.917623	1.741670	0.007690	0.702066
-40.867772	-1.866318	1.746675	0.007741	0.702072
-40.728784	-1.891226	1.751680	0.007715	0.702072
-40.833260	-1.906719	1.756685	0.007735	0.702003
-41.544720	-1.908024	1.761690	0.007867	0.701743
-41.628455	-1.896188	1.766694	0.007883	0.701737
-41.779892	-1.866726	1.771699	0.007911	0.701742
-41.493625	-1.917473	1.776704	0.007858	0.701742
-41.803901	-1.865010	1.781709	0.007916	0.701736
-42.108332	-1.806878	1.786714	0.007972	0.701744
-41.855078	-1.870753	1.791718	0.007925	0.701706
-42.533470	-1.884603	1.796723	0.008052	0.701433
-42.689010	-1.856376	1.801728	0.008080	0.701434
-42.878193	-1.825813	1.806733	0.008116	0.701428
-42.177912	-1.944257	1.811738	0.007985	0.701441
-42.648719	-1.865479	1.816742	0.008073	0.701430
-42.936989	-1.811040	1.821747	0.008127	0.701436
-42.459129	-1.901465	1.826752	0.008038	0.701426
-43.055999	-1.948176	1.831757	0.008149	0.701115
-43.505042	-1.863796	1.836762	0.008233	0.701124
-43.458096	-1.877071	1.841766	0.008224	0.701114
-43.232876	-1.915200	1.846771	0.008182	0.701118
-43.205927	-1.919014	1.851776	0.008177	0.701120
-43.441539	-1.879475	1.856781	0.008221	0.701115
-43.305789	-1.955980	1.861786	0.008196	0.701009
-44.538060	-1.807207	1.866790	0.008425	0.700865
-44.289831	-1.848979	1.871795	0.008379	0.700870
-43.869004	-1.921837	1.876800	0.008301	0.700875
-44.517694	-1.810329	1.881805	0.008421	0.700866
-44.304733	-1.843308	1.886810	0.008382	0.700876
-44.241232	-1.859880	1.891814	0.008370	0.700865
-44.214213	-1.962189	1.896819	0.008365	0.700668
-45.412920	-1.816320	1.901824	0.008588	0.700530
-45.182884	-1.858776	1.906829	0.008545	0.700527
-44.808188	-1.921640	1.911834	0.008476	0.700535
-45.382125	-1.822033	1.916838	0.008583	0.700530
-45.259272	-1.842219	1.921843	0.008560	0.700533
-44.900438	-1.907143	1.926848	0.008493	0.700531
-45.264979	-1.962785	1.931853	0.008561	0.700286
-46.048178	-1.855260	1.936858	0.008707	0.700221
-45.949262	-1.875989	1.941862	0.008688	0.700215
-45.785340	-1.904307	1.946867	0.008658	0.700217
-46.042153	-1.857403	1.951872	0.008706	0.700219
-46.153916	-1.840868	1.956877	0.008727	0.700212
-45.451087	-1.981916	1.961882	0.008596	0.700180
-46.787997	-1.886511	1.966886	0.008845	0.699890
-46.919089	-1.860604	1.971891	0.008869	0.699895
-46.652333	-1.909417	1.976896	0.008820	0.699892
-46.566153	-1.927142	1.981901	0.008804	0.699887
-46.672221	-1.904428	1.986906	0.008823	0.699895
-46.813858	-1.882179	1.991910	0.008850	0.699889
-46.836111	-1.950910	1.996915	0.008854	0.699741
-47.790330	-1.852075	2.001920	0.009032	0.699596
-47.490646	-1.905579	2.011917	0.008976	0.699596
-47.645237	-1.877375	2.021914	0.009005	0.699597
-47.824400	-1.845712	2.031910	0.009038	0.699597
-47.678528	-1.872786	2.041907	0.009011	0.699594
-47.643662	-1.877407	2.051904	0.009005	0.699597
-47.574596	-1.889743	2.061901	0.008992	0.699597
-47.708403	-1.865900	2.071898	0.009017	0.699597
-47.578956	-1.889814	2.081894	0.008993	0.699595
-47.737904	-1.862949	2.091891	0.009022	0.699592
-47.615532	-1.883522	2.101888	0.009000	0.699595
-47.675001	-1.871627	2.111885	0.009011	0.699597
-47.858296	-1.839882	2.121882	0.009045	0.699595
-47.781993	-1.811931	2.131878	0.009031	0.699679
-47.011332	-1.845805	2.141875	0.008887	0.699889
-47.057738	-1.835970	2.151872	0.008896	0.699892
-46.874034	-1.868211	2.161869	0.008862	0.699893
-46.975172	-1.849309	2.171866	0.008881	0.699895
-46.291274	-1.858620	2.181862	0.008754	0.700123
-46.129860	-1.842230	2.191859	0.008724	0.700215
-46.097529	-1.847785	2.201856	0.008718	0.700215
-45.837193	-1.894154	2.211853	0.008669	0.700215
-45.860372	-1.812350	2.221850	0.008673	0.700373
-44.958641	-1.894080	2.231846	0.008506	0.700533
-45.263538	-1.840383	2.241843	0.008562	0.700531
-45.097013	-1.869714	2.251840	0.008532	0.700532
-44.517574	-1.889283	2.261837	0.008424	0.700702
-44.210548	-1.859558	2.271834	0.008367	0.700873
-44.068362	-1.884624	2.281830	0.008340	0.700873
-44.321381	-1.841491	2.291827	0.008387	0.700869
-43.935902	-1.840202	2.301824	0.008316	0.701011
-43.305230	-1.899713	2.311821	0.008198	0.701118
-43.605801	-1.845285	2.321818	0.008254	0.701120
-43.480994	-1.847805	2.331814	0.008231	0.701159
-42.738179	-1.845899	2.341811	0.008093	0.701431
-42.414989	-1.903781	2.351808	0.008033	0.701431
-42.409737	-1.904390	2.361805	0.008032	0.701431
-42.273835	-1.844596	2.371802	0.008007	0.701601
-41.530271	-1.907889	2.381798	0.007868	0.701741
-41.997915	-1.826684	2.391795	0.007955	0.701737
-41.588634	-1.880335	2.401792	0.007879	0.701776
-40.890578	-1.859615	2.411789	0.007749	0.702070
-40.770331	-1.881038	2.421786	0.007727	0.702069
-40.903641	-1.857673	2.431782	0.007752	0.702068
-40.465946	-1.838818	2.441779	0.007670	0.702264
-40.052160	-1.863259	2.451776	0.007593	0.702364
-40.134847	-1.847183	2.461773	0.007609	0.702367
-39.810642	-1.867203	2.471770	0.007549	0.702443
-39.057720	-1.880597	2.481766	0.007408	0.702687
-39.223157	-1.851816	2.491763	0.007439	0.702685
-39.065182	-1.878727	2.501760	0.007410	0.702688
-38.657904	-1.830640	2.511757	0.007334	0.702932
-38.180639	-1.879813	2.521754	0.007245	0.703004
-38.422944	-1.837326	2.531750	0.007291	0.703002
-38.213253	-1.819244	2.541747	0.007252	0.703114
-37.346227	-1.863464	2.551744	0.007090	0.703337
-37.331924	-1.865183	2.561741	0.007088	0.703339
-37.536451	-1.828466	2.571738	0.007126	0.703339
-36.699134	-1.839195	2.581734	0.006970	0.703619
-36.658551	-1.840602	2.591731	0.006962	0.703630
-36.501965	-1.868037	2.601728	0.006933	0.703631
-36.443254	-1.791567	2.611725	0.006922	0.703806
-35.678430	-1.857163	2.621722	0.006780	0.703949
-35.685129	-1.856222	2.631718	0.006781	0.703948
-35.463486	-1.888938	2.641715	0.006740	0.703962
-34.836798	-1.854498	2.651712	0.006624	0.704257
-34.761694	-1.867404	2.661709	0.006610	0.704257
-34.655890	-1.886326	2.671706	0.006590	0.704257
-34.603522	-1.809071	2.681702	0.006580	0.704432
-33.976058	-1.843862	2.691699	0.006463	0.704587
-33.817755	-1.871872	2.701696	0.006434	0.704587
-33.839067	-1.868403	2.711693	0.006438	0.704586
-32.972853	-1.875360	2.721690	0.006277	0.704883
-32.922753	-1.883769	2.731686	0.006268	0.704884
-32.895477	-1.889661	2.741683	0.006263	0.704882
-32.867003	-1.848115	2.751680	0.006257	0.704976
-31.902617	-1.905561	2.761677	0.006078	0.705206
-32.026404	-1.883086	2.771674	0.006101	0.705207
-32.567009	-1.787858	2.781670	0.006202	0.705205
-31.421974	-1.847759	2.791667	0.005988	0.705495
-31.491085	-1.822643	2.801664	0.006001	0.705520
-31.192349	-1.874986	2.811661	0.005946	0.705522
-30.876428	-1.847074	2.821658	0.005887	0.705691
-30.468091	-1.834411	2.831654	0.005811	0.705863
-30.445710	-1.839548	2.841651	0.005807	0.705861
-30.367744	-1.853933	2.851648	0.005793	0.705860
-29.744212	-1.832265	2.861645	0.005677	0.706127
-29.524827	-1.870927	2.871642	0.005636	0.706127
-29.682105	-1.843378	2.881638	0.005665	0.706126
-29.068756	-1.858765	2.891635	0.005551	0.706315
-28.724461	-1.857278	2.901632	0.005487	0.706441
-28.835795	-1.836830	2.911629	0.005508	0.706442
-28.641321	-1.841413	2.921626	0.005472	0.706503
-27.986233	-1.833682	2.931622	0.005350	0.706753
-27.746443	-1.877964	2.941619	0.005305	0.706750
-28.045704	-1.824251	2.951616	0.005361	0.706750
-27.258776	-1.831916	2.961613	0.005214	0.707016
-27.159872	-1.817647	2.971610	0.005196	0.707080
-27.096891	-1.828348	2.981606	0.005184	0.707081
-26.623368	-1.859633	2.991603	0.005096	0.707188
-26.230382	-1.836871	3.001600	0.005023	0.707374
-25.936492	-1.888847	3.011597	0.004968	0.707375
-26.086908	-1.861589	3.021594	0.004996	0.707375
-25.437337	-1.839265	3.031590	0.004876	0.707652
-25.393853	-1.825530	3.041587	0.004868	0.707695
-25.334759	-1.834953	3.051584	0.004857	0.707697
-25.002778	-1.823655	3.061581	0.004795	0.707839
-24.327662	-1.856037	3.071578	0.004669	0.708015
-24.477305	-1.830867	3.081574	0.004697	0.708012
-24.317668	-1.860549	3.091571	0.004667	0.708009
-23.628484	-1.815707	3.101568	0.004539	0.708345
-23.207983	-1.888802	3.111565	0.004461	0.708349
-23.316676	-1.869567	3.121562	0.004481	0.708348
-23.399742	-1.816209	3.131558	0.004497	0.708425
-22.414566	-1.886956	3.141555	0.004313	0.708635
-22.459050	-1.878970	3.151552	0.004322	0.708635
-22.495945	-1.871322	3.161549	0.004329	0.708637
-21.940296	-1.863528	3.171546	0.004225	0.708851
-21.708391	-1.853826	3.181542	0.004182	0.708953
-21.631206	-1.867798	3.191539	0.004168	0.708953
-21.785924	-1.811825	3.201536	0.004197	0.709009
-20.640659	-1.888745	3.211533	0.003984	0.709264
-20.790501	-1.860889	3.221530	0.004011	0.709266
-20.649062	-1.888070	3.231526	0.003985	0.709262
-20.418190	-1.824753	3.241523	0.003942	0.709471
-19.993374	-1.840903	3.251520	0.003863	0.709590
-19.931519	-1.849134	3.261517	0.003852	0.709595
-19.941619	-1.820707	3.271514	0.003854	0.709649
-18.917755	-1.880983	3.281510	0.003663	0.709893
-18.996072	-1.867125	3.291507	0.003678	0.709892
-19.186982	-1.834022	3.301504	0.003713	0.709891
-18.603077	-1.825584	3.311501	0.003605	0.710115
-18.548929	-1.783791	3.321498	0.003595	0.710218
-18.154262	-1.855358	3.331494	0.003521	0.710215
-18.163417	-1.788704	3.341491	0.003523	0.710345
-17.351948	-1.841008	3.351488	0.003372	0.710529
-17.507613	-1.811332	3.361485	0.003401	0.710533
-17.200867	-1.864765	3.371482	0.003344	0.710536
-16.458290	-1.834935	3.381478	0.003206	0.710859
-16.487046	-1.824899	3.391475	0.003211	0.710869
-16.426380	-1.835574	3.401472	0.003200	0.710869
-16.208361	-1.820342	3.411469	0.003159	0.710977
-15.849194	-1.802254	3.421466	0.003093	0.711141
-15.477724	-1.868979	3.431462	0.003024	0.711140
-15.755803	-1.820505	3.441459	0.003075	0.711137
-14.671302	-1.856509	3.451456	0.002873	0.711451
-14.403732	-1.901349	3.461453	0.002824	0.711456
-14.192245	-1.939017	3.471450	0.002784	0.711456
-14.431375	-1.897210	3.481446	0.002829	0.711455
-13.790788	-1.858424	3.491443	0.002710	0.711759
-13.384153	-1.931374	3.501440	0.002634	0.711758
-13.502042	-1.908389	3.511437	0.002656	0.711762
-13.602996	-1.856709	3.521434	0.002675	0.711829
-12.615690	-1.902285	3.531430	0.002491	0.712089
-12.776732	-1.873140	3.541427	0.002521	0.712090
-12.636511	-1.899362	3.551424	0.002495	0.712087
-12.242238	-1.875582	3.561421	0.002422	0.712274
-11.826802	-1.893017	3.571418	0.002345	0.712387
-11.889504	-1.882337	3.581414	0.002356	0.712386
-11.795855	-1.891825	3.591411	0.002339	0.712400
-10.711436	-1.930212	3.601408	0.002137	0.712708
-10.852540	-1.904307	3.611405	0.002163	0.712710
-10.703057	-1.930295	3.621402	0.002136	0.712711
-10.726612	-1.894009	3.631398	0.002140	0.712775
-10.034164	-1.892510	3.641395	0.002011	0.713023
-9.919180	-1.911958	3.651392	0.001990	0.713025
-10.053811	-1.886931	3.661389	0.002015	0.713027
-9.352524	-1.907504	3.671386	0.001884	0.713235
-9.095032	-1.890034	3.681382	0.001837	0.713361
-9.108496	-1.888560	3.691379	0.001839	0.713359
-8.648537	-1.971514	3.701376	0.001754	0.713356
-8.487255	-1.870431	3.711373	0.001724	0.713615
-8.060421	-1.926218	3.721370	0.001644	0.713655
-8.181553	-1.906505	3.731366	0.001667	0.713651
-8.087133	-1.875902	3.741363	0.001649	0.713745
-7.231509	-1.916896	3.751360	0.001490	0.713966
-7.178428	-1.923464	3.761357	0.001480	0.713972
-6.926353	-1.969300	3.771354	0.001433	0.713970
-6.708425	-1.903683	3.781350	0.001393	0.714178
-6.393450	-1.910133	3.791347	0.001334	0.714276
-6.279770	-1.931942	3.801344	0.001313	0.714273
-6.288702	-1.912037	3.811341	0.001315	0.714309
-5.255161	-1.946843	3.821338	0.001122	0.714606
-5.404972	-1.918876	3.831334	0.001150	0.714608
-5.212116	-1.954161	3.841331	0.001115	0.714606
-5.281558	-1.890951	3.851328	0.001128	0.714707
-4.529476	-1.923293	3.861325	0.000988	0.714908
-4.602498	-1.909400	3.871322	0.001001	0.714910
-4.855333	-1.864733	3.881318	0.001048	0.714909
-3.916607	-1.870611	3.891315	0.000874	0.715229
-3.730757	-1.902678	3.901312	0.000839	0.715231
-3.638534	-1.918577	3.911309	0.000822	0.715232
-3.293074	-1.891325	3.921306	0.000758	0.715408
-2.915727	-1.889084	3.931302	0.000687	0.715546
-2.599634	-1.946204	3.941299	0.000629	0.715544
-2.682489	-1.932372	3.951296	0.000644	0.715542
-2.118961	-1.884503	3.961293	0.000539	0.715836
-1.820426	-1.914360	3.971290	0.000484	0.715882
-1.892768	-1.901850	3.981286	0.000497	0.715881
-1.797147	-1.878678	3.991283	0.000480	0.715961
-1.402775	-1.864539	4.001280	0.000406	0.716128
-1.467523	-1.851962	4.011277	0.000418	0.716130
-1.213529	-1.861406	4.021274	0.000371	0.716201
-1.354598	-1.713457	4.031270	0.000397	0.716444
-1.200767	-1.742301	4.041267	0.000369	0.716441
-1.002869	-1.670010	4.051264	0.000332	0.716653
-0.729469	-1.669458	4.061261	0.000281	0.716751
-0.633881	-1.644097	4.071258	0.000263	0.716835
-0.939847	-1.464533	4.081254	0.000320	0.717082
-0.818279	-1.449272	4.091251	0.000298	0.717155
-0.911004	-1.320203	4.101248	0.000315	0.717377
-1.002973	-1.221358	4.111245	0.000332	0.717540
-0.635525	-1.204046	4.121242	0.000264	0.717704
-0.632777	-1.074020	4.131238	0.000263	0.717962
-0.773208	-0.975219	4.141235	0.000289	0.718107
-0.679489	-0.868525	4.151232	0.000272	0.718351
-0.739406	-0.731931	4.161229	0.000283	0.718599
-0.564501	-0.664282	4.171226	0.000250	0.718794
-0.386902	-0.587064	4.181222	0.000217	0.719009
-0.448264	-0.443361	4.191219	0.000229	0.719271
-0.372409	-0.308549	4.201216	0.000215	0.719563
-0.399730	-0.183774	4.211213	0.000220	0.719799
-0.160446	-0.091524	4.221210	0.000175	0.720065
-0.192943	0.055130	4.231206	0.000181	0.720342
-0.162234	0.193877	4.241203	0.000175	0.720626
0.000000	0.349794	4.251200	0.000145	0.720990
0.152460	0.935033	4.256205	0.000116	0.722194
0.126100	2.208086	4.261210	0.000120	0.724681
0.236682	4.030399	4.266214	0.000099	0.728278
0.692033	6.359142	4.271219	0.000012	0.732956
1.189675	9.185419	4.276224	-0.000082	0.738576
1.200780	12.576284	4.281229	-0.000086	0.745064
1.512948	16.376558	4.286234	-0.000147	0.752369
1.985534	20.538375	4.291238	-0.000238	0.760332
2.265503	25.142761	4.296243	-0.000293	0.768966
2.804136	30.067627	4.301248	-0.000396	0.778172
3.302663	35.346170	4.306253	-0.000492	0.787894
3.774889	40.954281	4.311258	-0.000584	0.798075
4.212954	46.861317	4.316262	-0.000669	0.808642
4.648509	53.068308	4.321267	-0.000754	0.819590
6.390290	59.311752	4.326272	-0.001083	0.830850
7.477339	65.911693	4.331277	-0.001289	0.842365
7.721763	72.895398	4.336282	-0.001340	0.854114
7.997332	80.058625	4.341286	-0.001395	0.866007
8.355482	87.404702	4.346291	-0.001467	0.878057
8.804505	94.902433	4.351296	-0.001555	0.890211
10.184339	102.388542	4.356301	-0.001817	0.902440
12.235734	109.950486	4.361306	-0.002204	0.914804
12.488007	117.921885	4.366310	-0.002256	0.927147
13.180512	125.955009	4.371315	-0.002390	0.939537
13.798925	134.093322	4.376320	-0.002511	0.951902
14.924076	142.234207	4.381325	-0.002726	0.964243
15.324908	150.595237	4.386330	-0.002806	0.976563
16.972581	158.806345	4.391334	-0.003118	0.988825
25.138363	166.063259	4.396339	-0.004643	1.001192
25.437143	174.755322	4.401344	-0.004704	1.013498
25.784224	183.449957	4.406349	-0.004774	1.025671
26.017293	192.195795	4.411354	-0.004823	1.037744
26.102199	200.956416	4.416358	-0.004845	1.049663
26.833114	209.628741	4.421363	-0.004987	1.061480
27.851232	218.269275	4.426368	-0.005182	1.073190
28.171274	227.011464	4.431373	-0.005247	1.084748
29.594459	235.580246	4.436378	-0.005518	1.096206
30.401554	244.252278	4.441382	-0.005674	1.107541
30.862787	252.999340	4.446387	-0.005765	1.118780
31.355247	261.722483	4.451392	-0.005862	1.129884
32.529655	270.322631	4.456397	-0.006087	1.140872
33.399265	279.009604	4.461402	-0.006254	1.151797
33.923332	287.694934	4.466406	-0.006357	1.162546
35.283014	296.230510	4.471411	-0.006616	1.173186
36.343503	304.815529	4.476416	-0.006819	1.183729
36.794441	313.501470	4.481421	-0.006909	1.194175
37.357545	322.139641	4.486426	-0.007019	1.204496
37.809636	330.779567	4.491430	-0.007109	1.214709
39.038144	339.276776	4.496435	-0.007343	1.224824
39.929378	347.852267	4.501440	-0.007515	1.234879
40.902891	356.351116	4.506445	-0.007702	1.244782
42.095983	364.838570	4.511450	-0.007929	1.254635
42.623014	373.401273	4.516454	-0.008033	1.264369
43.239379	381.966319	4.521459	-0.008153	1.274048
43.686030	390.509323	4.526464	-0.008242	1.283597
44.149927	399.041829	4.531469	-0.008334	1.293068
45.520220	407.422715	4.536474	-0.008594	1.302470
46.120978	415.996188	4.541478	-0.008712	1.311873
46.895890	424.481291	4.546483	-0.008862	1.321145
47.306612	432.948930	4.551488	-0.008944	1.330268
47.923226	441.361602	4.556493	-0.009064	1.339308
48.767566	449.737648	4.561498	-0.009226	1.348288
49.293683	458.156994	4.566502	-0.009330	1.357198
50.024777	466.523040	4.571507	-0.009471	1.366030
50.861672	474.894731	4.576512	-0.009633	1.374829
51.795875	483.215760	4.581517	-0.009812	1.383536
52.308140	491.648169	4.586522	-0.009913	1.392230
52.914285	500.001742	4.591526	-0.010031	1.400806
53.195352	508.409304	4.596531	-0.010089	1.409330
54.123896	516.707596	4.601536	-0.010267	1.417800
54.848935	525.005206	4.606541	-0.010408	1.426186
55.337488	533.383245	4.611546	-0.010504	1.434563
55.979805	541.679958	4.616550	-0.010629	1.442836
56.867914	549.965940	4.621555	-0.010800	1.451091
57.150629	558.339454	4.626560	-0.010858	1.459287
57.487348	566.673867	4.631565	-0.010926	1.467408
57.980990	575.049258	4.636570	-0.011023	1.475549
58.690763	583.286478	4.641574	-0.011161	1.483546
59.457996	591.538709	4.646579	-0.011309	1.491523
59.969368	599.824121	4.651584	-0.011410	1.499450
60.490641	608.086541	4.656589	-0.011512	1.507314
61.208177	616.354186	4.661594	-0.011651	1.515173
61.764717	624.592064	4.666598	-0.011760	1.522938
62.102057	632.889663	4.671603	-0.011828	1.530686
62.722088	641.141844	4.676608	-0.011949	1.538395
63.394329	649.357577	4.681613	-0.012079	1.546040
63.996506	657.644361	4.686618	-0.012197	1.553702
64.357645	665.881566	4.691622	-0.012269	1.561245
64.995992	674.105673	4.696627	-0.012394	1.568781
65.812759	682.308342	4.701632	-0.012551	1.576287
66.516485	690.496380	4.706637	-0.012687	1.583727
67.179358	698.734240	4.711642	-0.012816	1.591171
67.677496	706.968213	4.716646	-0.012914	1.598554
68.000997	715.213337	4.721651	-0.012980	1.605887
68.568545	723.451750	4.726656	-0.013091	1.613215
69.389544	731.613064	4.731661	-0.013249	1.620478
69.712352	739.876231	4.736666	-0.013314	1.627728
70.218281	748.142893	4.741670	-0.013414	1.634974
70.655235	756.340905	4.746675	-0.013501	1.642119
71.169196	764.533791	4.751680	-0.013602	1.649238
71.379509	772.772679	4.756685	-0.013646	1.656325
72.193467	780.917069	4.761690	-0.013803	1.663384
72.959165	789.062283	4.766694	-0.013951	1.670406
73.546701	797.243336	4.771699	-0.014066	1.677405
74.242491	805.395477	4.776704	-0.014200	1.684364
74.927118	813.559455	4.781709	-0.014333	1.691304
75.421850	821.770874	4.786714	-0.014431	1.698229
75.614725	829.986355	4.791718	-0.014472	1.705090
75.930261	838.220373	4.796723	-0.014536	1.711954
76.381836	846.396853	4.801728	-0.014625	1.718761
76.939872	854.519890	4.806733	-0.014735	1.725511
77.538280	862.691543	4.811738	-0.014851	1.732280
78.089796	870.843524	4.816742	-0.014959	1.739000
78.481034	879.016924	4.821747	-0.015037	1.745691
79.116393	887.183555	4.826752	-0.015161	1.752381
79.613513	895.332282	4.831757	-0.015259	1.759015
79.833337	903.527707	4.836762	-0.015305	1.765625
80.144926	911.710299	4.841766	-0.015368	1.772213
80.697773	919.852604	4.846771	-0.015477	1.778773
81.238573	927.990011	4.851776	-0.015583	1.785304
81.577644	936.198958	4.856781	-0.015651	1.791843
81.904213	944.386847	4.861786	-0.015717	1.798340
82.539587	952.468530	4.866790	-0.015841	1.804767
83.016121	960.617396	4.871795	-0.015935	1.811205
83.499710	968.760576	4.876800	-0.016030	1.817616
83.954284	976.877528	4.881805	-0.016120	1.823981
84.606335	985.024168	4.886810	-0.016247	1.830370
84.803455	993.203844	4.891814	-0.016289	1.836707
85.391446	1001.301345	4.896819	-0.016403	1.843007
85.872836	1009.440211	4.901824	-0.016498	1.849303
86.038305	1017.611280	4.906829	-0.016534	1.855566
86.621042	1025.733564	4.911834	-0.016648	1.861819
87.184235	1033.844673	4.916838	-0.016758	1.868040
87.979924	1041.961733	4.921843	-0.016912	1.874272
88.549279	1050.065765	4.926848	-0.017023	1.880447
88.806704	1058.218025	4.931853	-0.017076	1.886602
89.141530	1066.393544	4.936858	-0.017144	1.892763
89.509249	1074.524014	4.941862	-0.017217	1.898875
90.159760	1082.594033	4.946867	-0.017344	1.904953
90.900027	1090.709087	4.951872	-0.017487	1.911056
90.995798	1098.898312	4.956877	-0.017510	1.917121
91.675589	1106.973202	4.961882	-0.017642	1.923148
92.157932	1115.090414	4.966886	-0.017737	1.929166
92.389649	1123.258143	4.971891	-0.017785	1.935174
92.516563	1131.422921	4.976896	-0.017814	1.941149
92.796715	1139.547446	4.981901	-0.017872	1.947094
93.358152	1147.686748	4.986906	-0.017982	1.953061
93.758606	1155.783298	4.991910	-0.018061	1.958962
94.485598	1163.817616	4.996915	-0.018202	1.964836
94.952291	1171.941162	5.001920	-0.018294	1.970728
95.236170	1180.067441	5.006925	-0.018352	1.976585
95.572395	1188.185788	5.011930	-0.018420	1.982424
96.033064	1196.271469	5.016934	-0.018511	1.988236
96.441351	1204.422436	5.021939	-0.018592	1.994072
96.755722	1212.517821	5.026944	-0.018656	1.999841
97.068763	1220.622458	5.031949	-0.018720	2.005600
97.833687	1228.693084	5.036954	-0.018867	2.011365
98.123354	1236.825520	5.041958	-0.018927	2.017108
98.568081	1244.904042	5.046963	-0.019015	2.022813
99.060883	1253.012089	5.051968	-0.019112	2.028527
99.170999	1261.185638	5.056973	-0.019137	2.034232
99.714375	1269.243801	5.061978	-0.019244	2.039884
100.173027	1277.312842	5.066982	-0.019334	2.045520
100.739611	1285.411322	5.071987	-0.019445	2.051171
101.133198	1293.527541	5.076992	-0.019524	2.056802
101.489021	1301.609736	5.081997	-0.019595	2.062389
101.884668	1309.722935	5.087002	-0.019674	2.067987
102.189610	1317.860472	5.092006	-0.019736	2.073577
102.612426	1325.934005	5.097011	-0.019820	2.079120
103.099118	1334.013929	5.102016	-0.019916	2.084659
103.209048	1342.132430	5.107021	-0.019942	2.090172
103.668119	1350.244239	5.112026	-0.020033	2.095701
104.149750	1358.306875	5.117030	-0.020127	2.101183
104.739556	1366.376235	5.122035	-0.020242	2.106667
105.146123	1374.530164	5.127040	-0.020323	2.112175
105.298676	1382.654504	5.132045	-0.020357	2.117624
106.133311	1390.660612	5.137050	-0.020518	2.123046
106.363609	1398.760250	5.142054	-0.020566	2.128458
106.717260	1406.877332	5.147059	-0.020637	2.133879
107.501950	1414.910751	5.152064	-0.020788	2.139273
107.762357	1422.995231	5.157069	-0.020842	2.144637
108.147895	1431.107638	5.162074	-0.020919	2.150017
108.871610	1439.161180	5.167078	-0.021059	2.155377
109.283746	1447.250949	5.172083	-0.021141	2.160718
109.400125	1455.379311	5.177088	-0.021168	2.166044
109.755930	1463.462789	5.182093	-0.021239	2.171349
110.262741	1471.554220	5.187098	-0.021339	2.176661
110.341537	1479.660584	5.192102	-0.021359	2.181929
110.745322	1487.737410	5.197107	-0.021439	2.187196
111.189718	1495.844962	5.202112	-0.021527	2.192473
111.604559	1503.897256	5.207117	-0.021610	2.197700
111.643329	1512.013370	5.212122	-0.021622	2.202920
112.114158	1520.066917	5.217126	-0.021715	2.208128
112.590588	1528.140754	5.222131	-0.021809	2.213336
112.913968	1536.225611	5.227136	-0.021875	2.218526
113.238732	1544.278158	5.232141	-0.021940	2.223682
113.666693	1552.365928	5.237146	-0.022025	2.228859
113.712970	1560.513430	5.242150	-0.022039	2.234027
113.862734	1568.587038	5.247155	-0.022072	2.239146
114.249899	1576.642385	5.252160	-0.022150	2.244262
114.540625	1584.706014	5.257165	-0.022209	2.249363
114.878311	1592.797805	5.262170	-0.022277	2.254475
115.256167	1600.859484	5.267174	-0.022353	2.259559
115.908240	1608.882041	5.272179	-0.022479	2.264632
116.309726	1617.007396	5.277184	-0.022559	2.269735
116.469179	1625.160982	5.282189	-0.022594	2.274823
117.024016	1633.176131	5.287194	-0.022703	2.279848
117.134966	1641.253731	5.292198	-0.022729	2.284863
117.129314	1649.348303	5.297203	-0.022733	2.289867
117.535229	1657.422691	5.302208	-0.022814	2.294882
117.939514	1665.438849	5.307213	-0.022894	2.299851
118.279392	1673.499790	5.312218	-0.022963	2.304831
118.685339	1681.565023	5.317222	-0.023043	2.309808
119.107123	1689.652676	5.322227	-0.023127	2.314790
119.709295	1697.684752	5.327232	-0.023245	2.319742
119.839846	1705.768487	5.332237	-0.023274	2.324675
120.175839	1713.853846	5.337242	-0.023342	2.329616
120.398590	1721.957846	5.342246	-0.023389	2.334548
120.565818	1730.019287	5.347251	-0.023425	2.339440
121.030304	1738.088711	5.352256	-0.023517	2.344350
121.646351	1746.127098	5.357261	-0.023637	2.349244
122.015258	1754.247294	5.362266	-0.023711	2.354156
122.435985	1762.285261	5.367270	-0.023794	2.359013
122.662043	1770.327722	5.372275	-0.023841	2.363847
123.098463	1778.391686	5.377280	-0.023928	2.368701
123.382158	1786.463947	5.382285	-0.023986	2.373538
123.787831	1794.532817	5.387290	-0.024067	2.378372
124.200562	1802.568500	5.392294	-0.024149	2.383177
124.296213	1810.664727	5.397299	-0.024172	2.387983
124.598607	1818.761055	5.402304	-0.024233	2.392796
124.863611	1826.802918	5.407309	-0.024288	2.397564
125.348791	1834.835601	5.412314	-0.024383	2.402335
125.756512	1842.891968	5.417318	-0.024465	2.407103
125.938525	1850.980744	5.422323	-0.024504	2.411864
126.358157	1859.054628	5.427328	-0.024587	2.416625
127.066182	1867.053029	5.432333	-0.024724	2.421355
127.522668	1875.121455	5.437338	-0.024814	2.426096
127.675085	1883.252862	5.442342	-0.024848	2.430842
128.101985	1891.361097	5.447347	-0.024933	2.435586
128.596712	1899.379493	5.452352	-0.025030	2.440273
128.962724	1907.391424	5.457357	-0.025103	2.444938
129.382944	1915.458035	5.462362	-0.025187	2.449630
129.789464	1923.528096	5.467366	-0.025268	2.454314
130.300628	1931.554798	5.472371	-0.025368	2.458971
130.623619	1939.623565	5.477376	-0.025434	2.463630
130.654612	1947.712424	5.482381	-0.025445	2.468269
131.122786	1955.779742	5.487386	-0.025537	2.472920
131.310479	1963.847636	5.492390	-0.025577	2.477542
131.370552	1971.906473	5.497395	-0.025594	2.482141
131.752971	1979.961258	5.502400	-0.025670	2.486752
132.132443	1988.008243	5.507405	-0.025746	2.491350
132.539327	1996.071759	5.512410	-0.025827	2.495951
133.055173	2004.107901	5.517414	-0.025928	2.500536
133.303639	2012.166509	5.522419	-0.025980	2.505105
133.770652	2020.232632	5.527424	-0.026072	2.509686
133.910367	2028.366719	5.532429	-0.026103	2.514274
134.441658	2036.372569	5.537434	-0.026207	2.518809
134.755235	2044.406613	5.542438	-0.026271	2.523336
135.019811	2052.443417	5.547443	-0.026325	2.527853
135.353132	2060.536042	5.552448	-0.026393	2.532398
135.821724	2068.558917	5.557453	-0.026485	2.536905
135.933366	2076.652231	5.562458	-0.026511	2.541418
136.286207	2084.676743	5.567462	-0.026582	2.545902
136.766066	2092.714138	5.572467	-0.026676	2.550394
136.961699	2100.833947	5.577472	-0.026718	2.554904
137.136966	2108.859160	5.582477	-0.026756	2.559352
137.441150	2116.896871	5.587482	-0.026818	2.563808
137.641129	2124.965039	5.592486	-0.026860	2.568266
137.943936	2133.040929	5.597491	-0.026922	2.572728
138.524456	2141.076153	5.602496	-0.027035	2.577178
138.680457	2149.119387	5.607501	-0.027069	2.581596
139.138675	2157.156861	5.612506	-0.027160	2.586024
139.415689	2165.240541	5.617510	-0.027217	2.590457
139.676296	2173.483031	5.622515	-0.027271	2.594968
139.760731	2181.490144	5.627520	-0.027292	2.599331
139.839232	2189.474987	5.632525	-0.027311	2.603674
140.353263	2197.476031	5.637530	-0.027412	2.608048
140.621229	2205.543341	5.642534	-0.027467	2.612434
140.795312	2213.585159	5.647539	-0.027505	2.616793
141.039120	2221.634753	5.652544	-0.027556	2.621153
141.340483	2229.647863	5.657549	-0.027617	2.625490
141.747914	2237.685710	5.662554	-0.027698	2.629840
142.082454	2245.744651	5.667558	-0.027766	2.634189
142.160126	2253.797744	5.672563	-0.027785	2.638511
142.716521	2261.809623	5.677568	-0.027894	2.642835
142.804327	2269.871716	5.682573	-0.027916	2.647149
143.055419	2277.936088	5.687578	-0.027968	2.651467
143.548465	2285.970667	5.692582	-0.028065	2.655777
143.863487	2293.992155	5.697587	-0.028128	2.660063
144.227296	2302.049666	5.702592	-0.028201	2.664363
144.694550	2310.087776	5.707597	-0.028294	2.668653
145.035563	2318.191064	5.712602	-0.028362	2.672962
145.468835	2326.218955	5.717606	-0.028448	2.677231
145.815770	2334.254385	5.722611	-0.028518	2.681491
146.183412	2342.305640	5.727616	-0.028592	2.685754
146.570608	2350.312868	5.732621	-0.028669	2.689988
147.423341	2358.370865	5.737626	-0.028833	2.694271
147.995770	2366.382328	5.742630	-0.028945	2.698505
148.325031	2374.441316	5.747635	-0.029011	2.702743
148.382744	2382.515830	5.752640	-0.029027	2.706964
148.794439	2390.574361	5.757645	-0.029109	2.711193
149.022297	2398.667708	5.762650	-0.029157	2.715422
149.246683	2406.678678	5.767654	-0.029204	2.719601
149.418578	2414.705356	5.772659	-0.029241	2.723778
150.078558	2422.740623	5.777664	-0.029369	2.727984
150.185432	2430.815158	5.782669	-0.029394	2.732169
150.533532	2438.884411	5.787674	-0.029464	2.736360
150.698452	2446.927985	5.792678	-0.029500	2.740520
151.081072	2454.925393	5.797683	-0.029577	2.744664
151.471606	2462.996741	5.802688	-0.029655	2.748839
151.461957	2471.144177	5.807693	-0.029658	2.753023
151.823931	2479.179256	5.812698	-0.029731	2.757165
152.004367	2487.202190	5.817702	-0.029769	2.761284
152.205984	2495.206620	5.822707	-0.029812	2.765388
152.700903	2503.207700	5.827712	-0.029910	2.769503
153.087230	2511.268592	5.832717	-0.029987	2.773635
153.620427	2519.298816	5.837722	-0.030091	2.777753
153.765492	2527.345286	5.842726	-0.030123	2.781851
154.061620	2535.379372	5.847731	-0.030184	2.785946
154.266233	2543.444707	5.852736	-0.030227	2.790045
154.530654	2551.510773	5.857741	-0.030282	2.794141
155.135477	2559.499979	5.862746	-0.030399	2.798213
155.287925	2567.555274	5.867750	-0.030433	2.802286
155.514253	2575.584092	5.872755	-0.030480	2.806344
155.967343	2583.630859	5.877760	-0.030570	2.810417
156.209646	2591.691393	5.882765	-0.030620	2.814480
156.372248	2599.746074	5.887770	-0.030656	2.818529
156.785014	2607.775679	5.892774	-0.030738	2.822574
157.114156	2615.812231	5.897779	-0.030804	2.826612
157.483578	2623.882769	5.902784	-0.030878	2.830664
157.680540	2631.944636	5.907789	-0.030920	2.834695
158.137658	2639.944588	5.912794	-0.031010	2.838705
158.184969	2648.004526	5.917798	-0.031024	2.842715
158.554518	2656.023626	5.922803	-0.031099	2.846718
158.836110	2664.075517	5.927808	-0.031156	2.850727
158.975042	2672.141137	5.932813	-0.031187	2.854728
159.312901	2680.168557	5.937818	-0.031255	2.858716
159.378018	2688.227324	5.942822	-0.031273	2.862699
159.712043	2696.242429	5.947827	-0.031340	2.866669
160.061573	2704.296284	5.952832	-0.031410	2.870654
160.129872	2712.347910	5.957837	-0.031428	2.874617
160.282812	2720.389776	5.962842	-0.031462	2.878574
160.511794	2728.431127	5.967846	-0.031510	2.882530
160.669038	2736.455920	5.972851	-0.031544	2.886468
161.142275	2744.484097	5.977856	-0.031638	2.890419
161.352116	2752.522695	5.982861	-0.031682	2.894356
161.591228	2760.578084	5.987866	-0.031732	2.898297
162.025040	2768.582623	5.992870	-0.031818	2.902219
162.171646	2776.641506	5.997875	-0.031850	2.906146
162.782070	2784.666042	6.002880	-0.031969	2.910076
162.814266	2792.822713	6.007885	-0.031980	2.914034
163.308398	2800.801731	6.012890	-0.032077	2.917925
163.455623	2808.829706	6.017894	-0.032110	2.921816
163.632276	2816.836791	6.022899	-0.032148	2.925693
164.167350	2824.840051	6.027904	-0.032253	2.929582
164.258719	2832.905869	6.032909	-0.032275	2.933473
164.548826	2840.953676	6.037914	-0.032334	2.937360
165.027074	2848.964554	6.042918	-0.032429	2.941234
165.282043	2856.965553	6.047923	-0.032481	2.945087
165.569740	2865.039470	6.052928	-0.032540	2.948971
165.851067	2873.088327	6.057933	-0.032598	2.952837
165.950780	2881.172711	6.062938	-0.032622	2.956706
166.213126	2889.188057	6.067942	-0.032676	2.960546
166.479822	2897.176788	6.072947	-0.032730	2.964368
166.702911	2905.251524	6.077952	-0.032777	2.968223
167.005631	2913.277107	6.082957	-0.032839	2.972055
167.406982	2921.315827	6.087962	-0.032919	2.975892
167.665183	2929.325084	6.092966	-0.032972	2.979704
168.043338	2937.340537	6.097971	-0.033048	2.983519
168.569113	2945.406901	6.102976	-0.033151	2.987361
168.780191	2953.466409	6.107981	-0.033195	2.991179
169.030508	2961.538799	6.112986	-0.033247	2.995000
169.193175	2969.548692	6.117990	-0.033283	2.998782
169.501895	2977.540763	6.122995	-0.033345	3.002559
169.929081	2985.597053	6.128000	-0.033430	3.006366
170.115241	2993.612595	6.133005	-0.033470	3.010138
170.261199	3001.703152	6.138010	-0.033502	3.013938
170.386781	3009.750761	6.143014	-0.033531	3.017712
170.564296	3017.766345	6.148019	-0.033569	3.021469
170.871624	3025.800530	6.153024	-0.033632	3.025236
171.091754	3033.822504	6.158029	-0.033678	3.028989
171.538491	3041.876584	6.163034	-0.033766	3.032763
172.177903	3049.897443	6.168038	-0.033890	3.036526
172.257513	3057.917337	6.173043	-0.033910	3.040257
172.444268	3065.957590	6.178048	-0.033950	3.043998
172.718878	3073.979228	6.183053	-0.034007	3.047729
173.066273	3082.025617	6.188058	-0.034077	3.051471
173.579365	3090.051525	6.193062	-0.034177	3.055207
174.072809	3098.058431	6.198067	-0.034274	3.058929
174.405471	3106.099941	6.203072	-0.034342	3.062654
174.210798	3114.179556	6.208077	-0.034311	3.066367
174.613883	3122.216715	6.213082	-0.034391	3.070084
174.857336	3130.337858	6.218086	-0.034441	3.073828
175.300032	3138.330376	6.223091	-0.034529	3.077518
175.877635	3146.312223	6.228096	-0.034642	3.081204
176.403704	3154.275722	6.233101	-0.034745	3.084875
176.585468	3162.330896	6.238106	-0.034784	3.088568
176.866332	3170.411119	6.243110	-0.034841	3.092272
177.059084	3178.436795	6.248115	-0.034883	3.095943
177.344259	3186.479268	6.253120	-0.034941	3.099622
177.153210	3194.544878	6.258125	-0.034911	3.103284
177.720053	3202.535846	6.263130	-0.035021	3.106943
178.033338	3210.596934	6.268134	-0.035085	3.110618
178.164443	3218.645934	6.273139	-0.035114	3.114275
178.420236	3226.673448	6.278144	-0.035167	3.117923
178.721759	3234.663161	6.283149	-0.035229	3.121552
178.949102	3242.675210	6.288154	-0.035276	3.125184
179.086518	3250.732578	6.293158	-0.035307	3.128828
179.120143	3258.784028	6.298163	-0.035318	3.132460
179.665857	3266.831164	6.303168	-0.035425	3.136108
179.651735	3274.830502	6.308173	-0.035428	3.139707
179.871494	3282.853609	6.313178	-0.035474	3.143322
180.146358	3290.911296	6.318182	-0.035530	3.146950
180.360664	3298.924423	6.323187	-0.035575	3.150552
180.690221	3307.010934	6.328192	-0.035642	3.154188
181.046580	3314.973741	6.333197	-0.035714	3.157765
181.354606	3323.014083	6.338202	-0.035776	3.161370
181.760020	3331.007425	6.343206	-0.035857	3.164955
181.662481	3339.078320	6.348211	-0.035844	3.168549
182.258984	3347.101848	6.353216	-0.035960	3.172147
182.506562	3355.152258	6.358221	-0.036011	3.175738
182.646667	3363.193415	6.363226	-0.036043	3.179316
183.016869	3371.213178	6.368230	-0.036117	3.182890
183.139871	3379.253136	6.373235	-0.036145	3.186459
183.343725	3387.299388	6.378240	-0.036188	3.190030
183.546592	3395.358389	6.383245	-0.036231	3.193602
183.791368	3403.370912	6.388250	-0.036282	3.197152
183.856963	3411.416567	6.393254	-0.036299	3.200705
184.122338	3419.378556	6.398259	-0.036354	3.204225
184.659687	3427.420203	6.403264	-0.036459	3.207788
184.939939	3435.480419	6.408269	-0.036517	3.211344
185.147440	3443.525281	6.413274	-0.036560	3.214887
185.285903	3451.549310	6.418278	-0.036591	3.218414
185.416452	3459.573694	6.423283	-0.036621	3.221936
185.525246	3467.601119	6.428288	-0.036646	3.225455
185.529268	3475.645018	6.433293	-0.036652	3.228973
186.065517	3483.686687	6.438298	-0.036757	3.232508
186.428612	3491.760699	6.443302	-0.036830	3.236047
186.610312	3499.714391	6.448307	-0.036869	3.239521
186.850514	3507.750206	6.453312	-0.036919	3.243030
187.039674	3515.765815	6.458317	-0.036960	3.246524
187.382770	3523.756547	6.463322	-0.037029	3.250010
187.852252	3531.817085	6.468326	-0.037121	3.253527
187.858517	3539.856370	6.473331	-0.037128	3.257013
188.056276	3547.892492	6.478336	-0.037170	3.260501
188.184245	3555.916993	6.483341	-0.037199	3.263978
188.610711	3563.939495	6.488346	-0.037283	3.267461
188.893069	3571.978112	6.493350	-0.037341	3.270943
189.089891	3580.001341	6.498355	-0.037383	3.274410
189.451255	3588.031306	6.503360	-0.037455	3.277884
189.588149	3596.091738	6.508365	-0.037486	3.281357
189.626271	3604.112299	6.513370	-0.037498	3.284807
190.030508	3612.130873	6.518374	-0.037579	3.288266
190.209337	3620.156515	6.523379	-0.037617	3.291715
190.433140	3628.214335	6.528384	-0.037664	3.295176
190.507689	3636.246673	6.533389	-0.037683	3.298617
190.739046	3644.242020	6.538394	-0.037732	3.302045
191.209553	3652.252996	6.543398	-0.037824	3.305485
191.436327	3660.259091	6.548403	-0.037872	3.308910
191.756214	3668.346675	6.553408	-0.037937	3.312369
192.051775	3676.385610	6.558413	-0.037997	3.315803
192.242748	3684.365900	6.563418	-0.038038	3.319205
192.441030	3692.398670	6.568422	-0.038080	3.322626
192.583496	3700.427806	6.573427	-0.038111	3.326040
192.851680	3708.466754	6.578432	-0.038167	3.329459
193.088918	3716.510912	6.583437	-0.038216	3.332875
193.291372	3724.567961	6.588442	-0.038259	3.336292
193.600013	3732.548749	6.593446	-0.038322	3.339677
193.661422	3740.566692	6.598451	-0.038338	3.343065
194.061391	3748.614507	6.603456	-0.038418	3.346475
194.436098	3756.615847	6.608461	-0.038493	3.349861
194.538906	3764.680865	6.613466	-0.038517	3.353260
194.865124	3772.763084	6.618470	-0.038583	3.356671
194.971330	3780.725413	6.623475	-0.038608	3.360021
195.332815	3788.750485	6.628480	-0.038681	3.363402
195.519104	3796.763057	6.633485	-0.038720	3.366769
195.908742	3804.783522	6.638490	-0.038798	3.370142
196.307449	3812.866679	6.643494	-0.038878	3.373539
196.334740	3820.909070	6.648499	-0.038888	3.376902
196.796919	3828.892681	6.653504	-0.038979	3.380253
196.809741	3836.911248	6.658509	-0.038987	3.383598
197.170763	3844.956320	6.663514	-0.039059	3.386964
197.325054	3852.982732	6.668518	-0.039093	3.390312
197.511935	3861.091763	6.673523	-0.039133	3.393691
197.882087	3869.103400	6.678528	-0.039207	3.397033
198.011957	3877.074745	6.683533	-0.039237	3.400347
198.308449	3885.053580	6.688538	-0.039297	3.403666
198.486752	3893.105982	6.693542	-0.039335	3.407009
198.522184	3901.127693	6.698547	-0.039347	3.410330
198.956341	3909.146100	6.703552	-0.039433	3.413661
199.388163	3917.184086	6.708557	-0.039519	3.416996
199.518862	3925.177022	6.713562	-0.039548	3.420299
199.734903	3933.248004	6.718566	-0.039594	3.423634
199.823437	3941.255533	6.723571	-0.039616	3.426935
200.117311	3949.263879	6.728576	-0.039675	3.430241
200.339062	3957.335375	6.733581	-0.039722	3.433566
200.620368	3965.345305	6.738586	-0.039780	3.436865
200.835673	3973.376051	6.743590	-0.039825	3.440167
200.893556	3981.390817	6.748595	-0.039841	3.443454
201.154946	3989.435703	6.753600	-0.039895	3.446757
201.432410	3997.454307	6.758605	-0.039952	3.450047
201.548497	4005.497522	6.763610	-0.039978	3.453338
201.870919	4013.545659	6.768614	-0.040044	3.456635
202.064687	4021.520835	6.773619	-0.040085	3.459895
202.427838	4029.582818	6.778624	-0.040158	3.463192
202.514699	4037.578042	6.783629	-0.040179	3.466450
202.627976	4045.619430	6.788634	-0.040205	3.469725
203.062092	4053.686816	6.793638	-0.040291	3.473018
203.161280	4061.741659	6.798643	-0.040315	3.476291
203.418874	4069.696147	6.803648	-0.040368	3.479526
203.788421	4077.697129	6.808653	-0.040442	3.482780
203.860094	4085.735359	6.813658	-0.040461	3.486036
204.005520	4093.768412	6.818662	-0.040493	3.489290
204.354589	4101.793109	6.823667	-0.040563	3.492544
204.588117	4109.834473	6.828672	-0.040612	3.495798
204.717759	4117.833448	6.833677	-0.040641	3.499028
204.972591	4125.851092	6.838682	-0.040694	3.502267
205.206244	4133.871715	6.843686	-0.040743	3.505503
205.179791	4141.909860	6.848691	-0.040743	3.508735
205.556833	4149.970184	6.853696	-0.040818	3.511986
205.848361	4157.982488	6.858701	-0.040878	3.515211
205.968277	4166.002209	6.863706	-0.040905	3.518432
206.087913	4174.068333	6.868710	-0.040933	3.521668
206.116037	4182.022532	6.873715	-0.040943	3.524853
206.589554	4190.045328	6.878720	-0.041037	3.528077
206.778398	4198.113701	6.883725	-0.041077	3.531307
206.849300	4206.147631	6.888730	-0.041095	3.534516
207.404068	4214.160208	6.893734	-0.041204	3.537729
207.574891	4222.163780	6.898739	-0.041241	3.540924
207.814013	4230.208760	6.903744	-0.041291	3.544134
207.987580	4238.237009	6.908749	-0.041328	3.547333
208.313686	4246.269055	6.913754	-0.041394	3.550535
208.285881	4254.446576	6.918758	-0.041394	3.553781
208.412990	4262.405904	6.923763	-0.041423	3.556943
208.692007	4270.388699	6.928768	-0.041480	3.560115
208.943617	4278.346070	6.933773	-0.041532	3.563273
209.059236	4286.347490	6.938778	-0.041559	3.566443
209.423503	4294.385999	6.943782	-0.041632	3.569631
209.656278	4302.406715	6.948787	-0.041680	3.572805
209.766543	4310.485591	6.953792	-0.041706	3.575996
209.923448	4318.457421	6.958797	-0.041741	3.579143
210.420364	4326.471872	6.963802	-0.041838	3.582315
210.529828	4334.509867	6.968806	-0.041864	3.585481
210.595383	4342.540725	6.973811	-0.041881	3.588640
211.098351	4350.581316	6.978816	-0.041980	3.591813
211.244898	4358.578511	6.983821	-0.042013	3.594956
211.241682	4366.605475	6.988826	-0.042017	3.598104
211.622130	4374.631937	6.993830	-0.042093	3.601259
211.981182	4382.577781	6.998835	-0.042165	3.604380
212.332305	4390.636658	7.003840	-0.042236	3.607541
212.356244	4398.690034	7.008845	-0.042246	3.610689
212.776589	4406.724787	7.013850	-0.042329	3.613837
213.056996	4414.778227	7.018854	-0.042386	3.616987
213.276720	4422.747724	7.023859	-0.042433	3.620099
213.456006	4430.773546	7.028864	-0.042471	3.623229
213.637535	4438.828718	7.033869	-0.042510	3.626368
213.897273	4446.840500	7.038874	-0.042564	3.629489
214.239642	4454.937990	7.043878	-0.042633	3.632643
214.574025	4462.936987	7.048883	-0.042700	3.635756
214.655177	4470.942809	7.053888	-0.042720	3.638862
214.823304	4478.960796	7.058893	-0.042757	3.641973
215.223629	4486.929383	7.063898	-0.042837	3.645067
215.336083	4494.996577	7.068902	-0.042863	3.648190
215.501889	4503.033944	7.073907	-0.042899	3.651300
215.754699	4511.082823	7.078912	-0.042951	3.654414
216.143975	4519.075953	7.083917	-0.043029	3.657507
215.967605	4527.109565	7.088922	-0.043001	3.660598
216.396653	4535.120274	7.093926	-0.043086	3.663694
216.871667	4543.104817	7.098931	-0.043180	3.666778
217.081289	4551.149912	7.103936	-0.043224	3.669876
217.311860	4559.212699	7.108941	-0.043272	3.672979
217.640799	4567.240020	7.113946	-0.043339	3.676068
217.990308	4575.266359	7.118950	-0.043409	3.679154
218.050361	4583.274828	7.123955	-0.043425	3.682224
218.232060	4591.281129	7.128960	-0.043464	3.685293
218.474875	4599.318734	7.133965	-0.043515	3.688373
218.698294	4607.329306	7.138970	-0.043562	3.691440
218.915506	4615.376503	7.143974	-0.043607	3.694518
219.082173	4623.381430	7.148979	-0.043644	3.697576
219.346550	4631.403887	7.153984	-0.043698	3.700641
219.691163	4639.399189	7.158989	-0.043767	3.703694
219.934774	4647.434073	7.163994	-0.043818	3.706758
220.155044	4655.468195	7.168998	-0.043864	3.709818
220.327290	4663.555730	7.174003	-0.043901	3.712895
220.620738	4671.610988	7.179008	-0.043961	3.715960
220.897628	4679.561279	7.184013	-0.044018	3.718982
220.903639	4687.583297	7.189018	-0.044024	3.722022
220.940686	4695.548041	7.194022	-0.044036	3.725039
221.164390	4703.559402	7.199027	-0.044083	3.728075
221.518506	4711.586483	7.204032	-0.044154	3.731118
221.532706	4719.656646	7.209037	-0.044162	3.734167
221.747156	4727.654598	7.214042	-0.044207	3.737191
222.017302	4735.653146	7.219046	-0.044263	3.740213
222.195379	4743.676488	7.224051	-0.044301	3.743241
222.191716	4751.715267	7.229056	-0.044306	3.746267
222.541972	4759.737699	7.234061	-0.044376	3.749293
222.626792	4767.788224	7.239066	-0.044397	3.752321
222.930542	4775.841738	7.244070	-0.044459	3.755353
223.179141	4783.798770	7.249075	-0.044510	3.758345
223.582771	4791.841024	7.254080	-0.044591	3.761370
223.755971	4799.835694	7.259085	-0.044628	3.764369
223.932184	4807.875016	7.264090	-0.044666	3.767383
224.265300	4815.958903	7.269094	-0.044733	3.770414
224.426422	4823.916155	7.274099	-0.044769	3.773392
224.505522	4832.021882	7.279104	-0.044789	3.776421
224.770605	4839.962251	7.284109	-0.044843	3.779390
224.939866	4848.004369	7.289114	-0.044880	3.782392
225.155381	4856.035099	7.294118	-0.044925	3.785389
225.380176	4864.041538	7.299123	-0.044972	3.788375
225.610595	4872.125432	7.304128	-0.045020	3.791387
225.690123	4880.168511	7.309133	-0.045040	3.794378
225.974217	4888.119267	7.314138	-0.045098	3.797337
226.258970	4896.128497	7.319142	-0.045157	3.800316
226.499974	4904.129864	7.324147	-0.045207	3.803288
226.802875	4912.171070	7.329152	-0.045268	3.806274
227.112649	4920.157588	7.334157	-0.045331	3.809237
227.198972	4928.205670	7.339162	-0.045352	3.812216
227.481307	4936.239441	7.344166	-0.045410	3.815192
227.709645	4944.221848	7.349171	-0.045458	3.818145
228.013237	4952.260372	7.354176	-0.045520	3.821118
228.094826	4960.246037	7.359181	-0.045540	3.824064
228.229529	4968.318781	7.364186	-0.045570	3.827042
228.620439	4976.312877	7.369190	-0.045648	3.829993
228.720034	4984.363811	7.374195	-0.045672	3.832957
228.870028	4992.386740	7.379200	-0.045705	3.835910
229.175081	5000.396979	7.384205	-0.045767	3.838859
229.492609	5008.413666	7.389210	-0.045831	3.841808
229.902550	5016.382092	7.394214	-0.045913	3.844739
230.119584	5024.420383	7.399219	-0.045959	3.847689
230.284403	5032.451643	7.404224	-0.045994	3.850633
230.383127	5040.519249	7.409229	-0.046018	3.853587
230.632324	5048.552330	7.414234	-0.046070	3.856529
231.113323	5056.525909	7.419238	-0.046164	3.859452
231.052810	5064.572215	7.424243	-0.046158	3.862388
231.139032	5072.589213	7.429248	-0.046180	3.865315
231.483222	5080.645416	7.434253	-0.046249	3.868258
231.788756	5088.667991	7.439258	-0.046311	3.871186
232.150828	5096.929713	7.444262	-0.046384	3.874200
232.021068	5104.880131	7.449267	-0.046365	3.877089
232.273423	5112.789290	7.454272	-0.046417	3.879968
232.429752	5120.791278	7.459277	-0.046451	3.882877
232.668465	5128.743310	7.464282	-0.046501	3.885767
233.134672	5136.781467	7.469286	-0.046593	3.888690
232.870125	5144.798135	7.474291	-0.046549	3.891590
233.125450	5152.832113	7.479296	-0.046601	3.894503
233.334107	5160.860861	7.484301	-0.046646	3.897412
233.715305	5168.800285	7.489306	-0.046722	3.900289
233.911032	5176.840998	7.494310	-0.046763	3.903197
233.966675	5184.896799	7.499315	-0.046779	3.906106
234.205670	5192.917984	7.504320	-0.046829	3.909003
234.468708	5200.963923	7.509325	-0.046883	3.911908
234.444878	5208.956100	7.514330	-0.046883	3.914786
234.995836	5216.979452	7.519334	-0.046991	3.917683
234.950013	5224.982919	7.524339	-0.046988	3.920561
235.260179	5232.962029	7.529344	-0.047051	3.923434
235.375043	5241.014400	7.534349	-0.047077	3.926327
235.687521	5249.014077	7.539354	-0.047141	3.929203
235.863702	5257.092791	7.544358	-0.047179	3.932103
236.217113	5265.089373	7.549363	-0.047250	3.934974
236.424592	5273.087872	7.554368	-0.047294	3.937841
236.496138	5281.113873	7.559373	-0.047312	3.940714
236.612021	5289.121739	7.564378	-0.047339	3.943579
236.915865	5297.170831	7.569382	-0.047401	3.946459
237.056678	5305.159556	7.574387	-0.047432	3.949313
237.222814	5313.218559	7.579392	-0.047468	3.952191
237.710066	5321.246886	7.584397	-0.047564	3.955061
237.789455	5329.247504	7.589402	-0.047584	3.957912
237.928700	5337.250170	7.594406	-0.047615	3.960763
238.236476	5345.261117	7.599411	-0.047678	3.963617
238.485252	5353.309795	7.604416	-0.047729	3.966482
238.483338	5361.298072	7.609421	-0.047734	3.969319
238.580177	5369.342830	7.614426	-0.047757	3.972176
238.882709	5377.347609	7.619430	-0.047819	3.975019
239.246635	5385.371233	7.624435	-0.047892	3.977869
239.303697	5393.373688	7.629440	-0.047908	3.980704
239.537249	5401.378062	7.634445	-0.047956	3.983540
239.811531	5409.437582	7.639450	-0.048013	3.986394
239.913838	5417.484438	7.644454	-0.048037	3.989239
240.144659	5425.513483	7.649459	-0.048085	3.992078
240.443901	5433.537244	7.654464	-0.048146	3.994914
240.710883	5441.526684	7.659469	-0.048201	3.997736
240.720248	5449.518530	7.664474	-0.048208	4.000552
241.141168	5457.576333	7.669478	-0.048291	4.003396
241.329602	5465.619461	7.674483	-0.048332	4.006228
241.403984	5473.605977	7.679488	-0.048351	4.009038
241.511123	5481.672227	7.684493	-0.048376	4.011873
241.665912	5489.664727	7.689498	-0.048410	4.014682
241.934104	5497.705053	7.694502	-0.048465	4.017507
241.892839	5505.671270	7.699507	-0.048463	4.020299
242.382232	5513.701730	7.704512	-0.048559	4.023120
242.744299	5521.755201	7.709517	-0.048632	4.025945
242.845223	5529.763363	7.714522	-0.048656	4.028749
243.001053	5537.795320	7.719526	-0.048690	4.031559
243.337617	5545.927070	7.724531	-0.048758	4.034405
243.460031	5553.903041	7.729536	-0.048786	4.037192
243.417105	5561.842410	7.734541	-0.048783	4.039961
243.881266	5569.821186	7.739546	-0.048874	4.042749
244.255448	5577.871337	7.744550	-0.048949	4.045559
244.114318	5585.881685	7.749555	-0.048928	4.048346
244.346925	5593.901573	7.754560	-0.048977	4.051140
244.581551	5601.928813	7.759565	-0.049026	4.053934
244.569852	5609.965641	7.764570	-0.049029	4.056726
244.979255	5617.923124	7.769574	-0.049110	4.059495
245.180505	5625.942496	7.774579	-0.049153	4.062280
245.342076	5633.951072	7.779584	-0.049188	4.065059
245.588359	5642.008622	7.784589	-0.049239	4.067854
245.818436	5650.003025	7.789594	-0.049287	4.070625
246.322525	5658.048781	7.794598	-0.049386	4.073416
246.280970	5666.075231	7.799603	-0.049384	4.076190
246.269323	5674.030016	7.804608	-0.049387	4.078938
246.815294	5682.108173	7.809613	-0.049493	4.081735
247.019440	5690.063537	7.814618	-0.049537	4.084483
247.362622	5698.138431	7.819622	-0.049606	4.087272
247.527325	5706.098190	7.824627	-0.049642	4.090016
248.066651	5714.151244	7.829632	-0.049747	4.092797
248.202524	5722.196627	7.834637	-0.049778	4.095567
248.391166	5730.172822	7.839642	-0.049818	4.098312
248.781670	5738.253029	7.844646	-0.049896	4.101094
248.962133	5746.215958	7.849651	-0.049935	4.103830
249.140458	5754.258084	7.854656	-0.049973	4.106592
249.397540	5762.269028	7.859661	-0.050026	4.109343
249.505110	5770.309309	7.864666	-0.050051	4.112100
249.757564	5778.392473	7.869670	-0.050104	4.114871
250.077334	5786.367357	7.874675	-0.050168	4.117604
250.201647	5794.324790	7.879680	-0.050197	4.120327
250.237925	5802.389480	7.884685	-0.050209	4.123084
250.328550	5810.390845	7.889690	-0.050231	4.125818
250.723509	5818.440445	7.894694	-0.050309	4.128570
250.822604	5826.469699	7.899699	-0.050333	4.131310
251.147796	5834.489757	7.904704	-0.050399	4.134048
251.452716	5842.530671	7.909709	-0.050461	4.136791
251.410331	5850.494956	7.914714	-0.050458	4.139501
251.535222	5858.564088	7.919718	-0.050487	4.142248
251.657804	5866.529394	7.924723	-0.050515	4.144957
251.839791	5874.565909	7.929728	-0.050554	4.147689
251.914037	5882.606050	7.934733	-0.050573	4.150420
252.007748	5890.624153	7.939738	-0.050595	4.153141
252.305382	5898.635912	7.944742	-0.050656	4.155861
252.313518	5906.627045	7.949747	-0.050663	4.158569
252.514897	5914.661992	7.954752	-0.050705	4.161292
252.754238	5922.666855	7.959757	-0.050755	4.164003
252.829192	5930.684437	7.964762	-0.050774	4.166715
253.068549	5938.722095	7.969766	-0.050824	4.169434
253.198726	5946.770598	7.974771	-0.050854	4.172154
253.735037	5954.772076	7.979776	-0.050959	4.174860
253.842959	5962.786620	7.984781	-0.050984	4.177565
253.797016	5970.749372	7.989786	-0.050980	4.180248
254.102631	5978.801271	7.994790	-0.051043	4.182964
254.169546	5986.818023	7.999795	-0.051060	4.185663
254.304293	5994.818304	8.004800	-0.051091	4.188356
254.611224	6002.875883	8.009805	-0.051153	4.191068
254.800202	6010.958370	8.014810	-0.051193	4.193785
254.946862	6019.005663	8.019814	-0.051226	4.196488
255.084353	6026.925398	8.024819	-0.051257	4.199147
255.308069	6034.933210	8.029824	-0.051303	4.201834
255.561931	6042.928537	8.034829	-0.051356	4.204516
255.504557	6050.916294	8.039834	-0.051350	4.207191
255.955006	6058.950481	8.044838	-0.051439	4.209884
255.966853	6066.989352	8.049843	-0.051447	4.212573
256.139173	6074.995813	8.054848	-0.051484	4.215250
256.510894	6083.000515	8.059853	-0.051559	4.217928
256.727101	6090.975811	8.064858	-0.051604	4.220592
257.077373	6099.045884	8.069862	-0.051674	4.223288
256.995811	6107.065604	8.074867	-0.051664	4.225960
257.077417	6115.061226	8.079872	-0.051685	4.228625
257.319762	6123.128544	8.084877	-0.051735	4.231313
257.403983	6131.140905	8.089882	-0.051756	4.233980
257.876761	6139.210137	8.094886	-0.051849	4.236668
258.085028	6147.103335	8.099891	-0.051893	4.239293
258.177349	6155.204155	8.104896	-0.051916	4.241984
258.401137	6163.169089	8.109901	-0.051962	4.244630
258.641730	6171.197939	8.114906	-0.052012	4.247295
258.575159	6179.200881	8.119910	-0.052005	4.249947
258.632722	6187.284576	8.124915	-0.052021	4.252625
259.107410	6195.264836	8.129920	-0.052115	4.255272
259.438759	6203.344772	8.134925	-0.052182	4.257948
259.225103	6211.319933	8.139930	-0.052147	4.260583
259.467253	6219.375660	8.144934	-0.052197	4.263247
259.791416	6227.330326	8.149939	-0.052263	4.265876
259.739095	6235.416355	8.154944	-0.052258	4.268544
260.118492	6243.413758	8.159949	-0.052334	4.271185
260.273499	6251.478946	8.164954	-0.052368	4.273845
260.479601	6259.489131	8.169958	-0.052412	4.276485
260.549050	6267.432906	8.174963	-0.052430	4.279101
260.892895	6275.505612	8.179968	-0.052499	4.281760
261.373547	6283.466054	8.184973	-0.052594	4.284381
261.463503	6291.508817	8.189978	-0.052616	4.287024
261.829783	6299.488871	8.194982	-0.052689	4.289648
261.989729	6307.579914	8.199987	-0.052724	4.292304
262.006890	6315.582398	8.204992	-0.052733	4.294929
262.314702	6323.598001	8.209997	-0.052795	4.297559
262.504408	6331.562371	8.215002	-0.052836	4.300169
262.537704	6339.610754	8.220006	-0.052847	4.302804
262.745467	6347.617968	8.225011	-0.052891	4.305425
262.939560	6355.623788	8.230016	-0.052932	4.308044
263.264028	6363.693661	8.235021	-0.052998	4.310683
263.347158	6371.695758	8.240026	-0.053019	4.313297
263.331301	6379.715536	8.245030	-0.053021	4.315914
263.609691	6387.716285	8.250035	-0.053078	4.318526
263.602433	6395.712123	8.255040	-0.053082	4.321132
263.830948	6403.703709	8.260045	-0.053129	4.323737
264.123878	6411.741960	8.265050	-0.053189	4.326356
264.666351	6419.764394	8.270054	-0.053295	4.328970
264.748163	6427.783638	8.275059	-0.053316	4.331578
264.863082	6435.805122	8.280064	-0.053342	4.334186
265.138535	6443.881924	8.285069	-0.053399	4.336811
265.145217	6451.794289	8.290074	-0.053405	4.339379
265.281467	6459.904082	8.295078	-0.053436	4.342011
265.674690	6467.858442	8.300083	-0.053514	4.344592
265.830021	6475.861131	8.305088	-0.053548	4.347186
266.055311	6483.935729	8.310093	-0.053595	4.349801
266.163062	6491.961674	8.315098	-0.053621	4.352399
266.295323	6500.058609	8.320102	-0.053651	4.355019
266.141512	6508.024081	8.325107	-0.053627	4.357592
266.641432	6515.965974	8.330112	-0.053725	4.360161
266.813013	6523.996496	8.335117	-0.053763	4.362754
266.762939	6531.934477	8.340122	-0.053758	4.365315
266.849131	6540.019807	8.345126	-0.053780	4.367922
267.159806	6548.010828	8.350131	-0.053843	4.370499
267.127445	6556.052819	8.355136	-0.053842	4.373089
267.157321	6564.082904	8.360141	-0.053853	4.375674
267.483082	6572.059956	8.365146	-0.053918	4.378241
267.675937	6580.119989	8.370150	-0.053960	4.380834
267.705413	6588.107107	8.375155	-0.053970	4.383400
267.814705	6596.089741	8.380160	-0.053996	4.385964
268.241059	6604.159170	8.385165	-0.054080	4.388556
268.222078	6612.158434	8.390170	-0.054082	4.391121
268.506279	6620.198145	8.395174	-0.054140	4.393699
268.763539	6628.248027	8.400179	-0.054193	4.396279
268.946150	6636.203514	8.405184	-0.054232	4.398827
268.923416	6644.279308	8.410189	-0.054233	4.401411
268.899900	6652.227039	8.415194	-0.054234	4.403952
269.426692	6660.290736	8.420198	-0.054338	4.406532
269.366349	6668.266003	8.425203	-0.054331	4.409079
269.545850	6676.279292	8.430208	-0.054370	4.411638
270.089290	6684.339661	8.435213	-0.054476	4.414212
270.243379	6692.367797	8.440218	-0.054510	4.416772
270.303058	6700.370718	8.445222	-0.054527	4.419323
270.450412	6708.414255	8.450227	-0.054559	4.421885
270.736806	6716.351573	8.455232	-0.054618	4.424412
271.002235	6724.462719	8.460237	-0.054672	4.426994
271.154505	6732.433956	8.465242	-0.054706	4.429528
271.370589	6740.519017	8.470246	-0.054751	4.432098
271.365205	6748.533256	8.475251	-0.054756	4.434643
271.670474	6756.556712	8.480256	-0.054818	4.437190
271.807900	6764.472953	8.485261	-0.054848	4.439702
272.104968	6772.526588	8.490266	-0.054909	4.442256
272.374947	6780.505491	8.495270	-0.054964	4.444785
272.484756	6788.557203	8.500275	-0.054990	4.447334
272.609600	6796.565038	8.505280	-0.055018	4.449869
272.951397	6804.638967	8.510285	-0.055087	4.452424
273.079429	6812.574079	8.515290	-0.055116	4.454932
273.244631	6820.660573	8.520294	-0.055152	4.457487
273.365494	6828.645477	8.525299	-0.055180	4.460008
273.568852	6836.624090	8.530304	-0.055223	4.462527
273.948485	6844.643886	8.535309	-0.055299	4.465057
274.185510	6852.659107	8.540314	-0.055348	4.467584
274.189425	6860.726181	8.545318	-0.055354	4.470125
274.287959	6868.758130	8.550323	-0.055378	4.472654
274.629478	6876.754339	8.555328	-0.055447	4.475171
274.751593	6884.808161	8.560333	-0.055474	4.477704
274.582248	6892.743418	8.565338	-0.055448	4.480197
275.078383	6900.748849	8.570343	-0.055546	4.482713
275.171468	6908.780908	8.575347	-0.055568	4.485235
275.163930	6916.781687	8.580352	-0.055572	4.487745
275.377636	6924.827655	8.585357	-0.055617	4.490268
275.522301	6932.846005	8.590362	-0.055649	4.492781
275.695518	6940.880611	8.595367	-0.055687	4.495298
275.808122	6948.897397	8.600371	-0.055713	4.497808
276.178938	6956.876510	8.605376	-0.055787	4.500305
276.275437	6964.928489	8.610381	-0.055810	4.502823
276.382555	6972.881002	8.615386	-0.055835	4.505309
276.566088	6980.932316	8.620391	-0.055875	4.507824
276.758241	6988.946119	8.625395	-0.055916	4.510326
276.723023	6997.003273	8.630400	-0.055914	4.512839
277.012571	7005.087473	8.635405	-0.055973	4.515361
277.183028	7013.004832	8.640410	-0.056010	4.517828
277.378425	7021.019663	8.645415	-0.056052	4.520325
277.520211	7029.022332	8.650419	-0.056083	4.522816
277.611894	7036.968589	8.655424	-0.056106	4.525289
277.720619	7045.045670	8.660429	-0.056131	4.527800
277.711041	7053.030575	8.665434	-0.056135	4.530282
278.122387	7061.076542	8.670439	-0.056216	4.532781
278.224477	7069.133026	8.675443	-0.056241	4.535282
278.332875	7077.131559	8.680448	-0.056266	4.537764
278.564202	7085.157992	8.685453	-0.056314	4.540253
278.801260	7093.126420	8.690458	-0.056364	4.542723
278.921817	7101.124100	8.695463	-0.056391	4.545200
279.131291	7109.196362	8.700467	-0.056435	4.547700
279.193409	7117.168902	8.705472	-0.056452	4.550166
279.337187	7125.253478	8.710477	-0.056484	4.552666
279.387740	7133.221726	8.715482	-0.056499	4.555129
279.577795	7141.295823	8.720487	-0.056539	4.557623
279.969700	7149.245121	8.725491	-0.056617	4.560078
279.859276	7157.322296	8.730496	-0.056602	4.562570
280.021695	7165.305611	8.735501	-0.056638	4.565032
280.241129	7173.309318	8.740506	-0.056684	4.567499
280.437332	7181.318536	8.745511	-0.056725	4.569966
280.499881	7189.370121	8.750515	-0.056742	4.572445
280.834477	7197.338019	8.755520	-0.056810	4.574897
281.115753	7205.442488	8.760525	-0.056867	4.577390
281.373926	7213.373749	8.765530	-0.056920	4.579828
281.362618	7221.418757	8.770535	-0.056924	4.582299
281.807473	7229.396934	8.775539	-0.057012	4.584749
281.754406	7237.419221	8.780544	-0.057007	4.587210
281.781448	7245.480280	8.785549	-0.057017	4.589683
281.940701	7253.492517	8.790554	-0.057052	4.592139
282.462909	7261.563649	8.795559	-0.057154	4.594612
282.598068	7269.595952	8.800563	-0.057185	4.597071
282.594049	7277.519491	8.805568	-0.057189	4.599496
282.916687	7285.603159	8.810573	-0.057255	4.601969
282.848154	7293.500526	8.815578	-0.057247	4.604383
283.347517	7301.586770	8.820583	-0.057345	4.606854
283.581117	7309.570245	8.825587	-0.057394	4.609292
283.314684	7317.609220	8.830592	-0.057349	4.611745
283.674286	7325.648386	8.835597	-0.057422	4.614198
283.782899	7333.660135	8.840602	-0.057447	4.616640
283.966315	7341.670070	8.845607	-0.057486	4.619081
284.216432	7349.687446	8.850611	-0.057538	4.621523
284.190727	7357.661716	8.855616	-0.057538	4.623950
284.379029	7365.727665	8.860621	-0.057579	4.626404
284.371061	7373.664208	8.865626	-0.057582	4.628817
284.581697	7381.756276	8.870631	-0.057627	4.631277
284.885206	7389.796351	8.875635	-0.057689	4.633719
284.902199	7397.779556	8.880640	-0.057697	4.636142
285.121097	7405.771495	8.885645	-0.057743	4.638567
285.507981	7413.785599	8.890650	-0.057820	4.640997
285.708802	7421.807719	8.895655	-0.057863	4.643429
285.846749	7429.814375	8.900659	-0.057894	4.645854
285.920130	7437.802399	8.905664	-0.057912	4.648273
286.121197	7445.851768	8.910669	-0.057955	4.650709
286.185816	7453.902931	8.915674	-0.057972	4.653144
286.403877	7461.894832	8.920679	-0.058018	4.655560
286.667761	7469.915949	8.925683	-0.058072	4.657983
286.890257	7477.883285	8.930688	-0.058119	4.660389
286.875086	7485.961467	8.935693	-0.058121	4.662827
287.146346	7493.918809	8.940698	-0.058177	4.665227
287.314898	7501.946188	8.945703	-0.058214	4.667647
287.429415	7509.932998	8.950707	-0.058240	4.670054
287.761964	7518.051521	8.955712	-0.058307	4.672499
288.012441	7526.190620	8.960717	-0.058359	4.674949
288.121065	7534.094639	8.965722	-0.058385	4.677327
288.174004	7542.039810	8.970727	-0.058400	4.679716
288.234779	7550.081579	8.975731	-0.058416	4.682133
288.269203	7557.942355	8.980736	-0.058428	4.684495
288.583447	7566.118721	8.985741	-0.058491	4.686949
288.649001	7574.045104	8.990746	-0.058509	4.689328
288.850400	7582.111756	8.995751	-0.058552	4.691747
288.988544	7590.159324	9.000755	-0.058582	4.694159
289.057517	7598.141840	9.005760	-0.058600	4.696551
289.281823	7606.168124	9.010765	-0.058647	4.698954
289.461386	7614.171166	9.015770	-0.058686	4.701350
289.712114	7622.193504	9.020775	-0.058738	4.703749
289.968511	7630.198155	9.025779	-0.058791	4.706142
290.122533	7638.230224	9.030784	-0.058825	4.708542
290.132172	7646.248584	9.035789	-0.058832	4.710938
290.229805	7654.261294	9.040794	-0.058855	4.713330
290.692112	7662.283256	9.045799	-0.058946	4.715722
290.453418	7670.301397	9.050803	-0.058907	4.718114
290.605579	7678.244182	9.055808	-0.058941	4.720482
291.160228	7686.365451	9.060813	-0.059049	4.722900
291.242544	7694.323209	9.065818	-0.059070	4.725270
291.242323	7702.329345	9.070823	-0.059075	4.727653
291.519106	7710.385202	9.075827	-0.059132	4.730049
291.714322	7718.339442	9.080832	-0.059173	4.732413
291.877567	7726.401452	9.085837	-0.059209	4.734809
291.834632	7734.440302	9.090842	-0.059206	4.737197
292.148579	7742.432179	9.095847	-0.059270	4.739569
292.249387	7750.473307	9.100851	-0.059293	4.741954
292.247477	7758.400564	9.105856	-0.059298	4.744306
292.780602	7766.511395	9.110861	-0.059403	4.746708
292.768597	7774.448716	9.115866	-0.059406	4.749060
292.947150	7782.515496	9.120871	-0.059444	4.751448
293.115070	7790.618996	9.125875	-0.059481	4.753846
293.192792	7798.541942	9.130880	-0.059500	4.756190
293.515402	7806.550942	9.135885	-0.059566	4.758557
293.591251	7814.552635	9.140890	-0.059585	4.760922
293.785588	7822.525965	9.145895	-0.059626	4.763276
293.752131	7830.604141	9.150899	-0.059625	4.765662
293.471002	7838.560479	9.155904	-0.059578	4.768011
293.985700	7846.651543	9.160909	-0.059679	4.770395
293.965645	7854.650920	9.165914	-0.059681	4.772754
294.439499	7862.667141	9.170919	-0.059774	4.775114
294.532770	7870.653783	9.175923	-0.059797	4.777466
294.643368	7878.614937	9.180928	-0.059822	4.779809
294.762952	7886.718149	9.185933	-0.059850	4.782192
294.810873	7894.652427	9.190938	-0.059864	4.784525
295.165270	7902.749004	9.195943	-0.059935	4.786904
295.234821	7910.708532	9.200947	-0.059953	4.789242
295.318144	7918.767898	9.205952	-0.059974	4.791608
295.872170	7926.835053	9.210957	-0.060082	4.793973
295.840552	7934.836962	9.215962	-0.060082	4.796321
295.906368	7942.740954	9.220967	-0.060099	4.798638
295.932375	7950.820812	9.225971	-0.060109	4.801006
296.018264	7958.797931	9.230976	-0.060130	4.803342
296.157249	7966.815009	9.235981	-0.060161	4.805688
296.568622	7974.830806	9.240986	-0.060243	4.808032
296.886485	7982.826747	9.245991	-0.060307	4.810369
296.920747	7990.456745	9.250995	-0.060319	4.812599
296.986804	7995.162855	9.256000	-0.060334	4.813974
297.070839	7997.771605	9.261005	-0.060351	4.814736
297.118228	7999.076226	9.266010	-0.060361	4.815117
297.126761	7999.550903	9.271015	-0.060363	4.815256
297.269333	8000.016057	9.276019	-0.060390	4.815391
297.480465	8000.503741	9.281024	-0.060429	4.815532
297.520763	8000.421035	9.286029	-0.060437	4.815508
297.414064	8000.502635	9.291034	-0.060417	4.815532
297.744387	8000.529485	9.296039	-0.060478	4.815538
297.900991	8000.361058	9.301043	-0.060507	4.815488
297.867684	8000.394707	9.306048	-0.060501	4.815498
297.944288	8000.366046	9.311053	-0.060515	4.815490
298.014039	8000.461260	9.316058	-0.060529	4.815517
298.096865	8000.338641	9.321063	-0.060544	4.815481
298.163477	8000.350431	9.326067	-0.060556	4.815484
298.083053	8000.380093	9.331072	-0.060541	4.815493
298.114754	8000.201046	9.336077	-0.060547	4.815441
298.053746	8000.372120	9.341082	-0.060536	4.815491
298.290760	8000.388872	9.346087	-0.060580	4.815495
298.294948	8000.518274	9.351091	-0.060581	4.815532
298.059918	8000.520788	9.356096	-0.060537	4.815534
298.350605	8000.240214	9.361101	-0.060591	4.815451
298.509264	8000.420275	9.366106	-0.060620	4.815503
298.505462	8000.392418	9.371111	-0.060620	4.815495
298.406730	8000.383297	9.376115	-0.060601	4.815493
298.540649	8000.528745	9.381120	-0.060626	4.815534
298.820939	8000.246927	9.386125	-0.060678	4.815451
298.576984	8000.486587	9.391130	-0.060633	4.815522
298.703073	8000.211833	9.396135	-0.060656	4.815441
298.808268	8000.419869	9.401139	-0.060676	4.815501
298.808519	8000.521416	9.406144	-0.060676	4.815531
298.935772	8000.497870	9.411149	-0.060700	4.815523
298.960790	8000.259918	9.416154	-0.060704	4.815454
298.862638	8000.511616	9.421159	-0.060686	4.815528
298.950656	8000.402977	9.426163	-0.060702	4.815496
298.862099	8000.211243	9.431168	-0.060686	4.815440
299.153696	8000.179732	9.436173	-0.060740	4.815429
298.889053	8000.484252	9.441178	-0.060691	4.815520
299.053187	8000.327706	9.446183	-0.060721	4.815473
299.219896	8000.333674	9.451187	-0.060752	4.815474
299.368817	8000.204666	9.456192	-0.060780	4.815436
299.581637	8000.330047	9.461197	-0.060819	4.815471
299.632432	8000.249650	9.466202	-0.060829	4.815448
299.553880	8000.365924	9.471207	-0.060814	4.815482
299.323176	8000.389887	9.476211	-0.060771	4.815490
299.346862	8000.427689	9.481216	-0.060776	4.815501
299.602221	8000.382752	9.486221	-0.060823	4.815487
299.449681	8000.395184	9.491226	-0.060795	4.815491
299.510599	8000.334195	9.496231	-0.060806	4.815473
299.645135	8000.213499	9.501235	-0.060831	4.815437
299.682073	8000.417202	9.506240	-0.060838	4.815496
299.816335	8000.202437	9.511245	-0.060863	4.815433
299.738602	8000.391411	9.516250	-0.060848	4.815488
299.682066	8000.355197	9.521255	-0.060838	4.815478
299.573214	8000.340562	9.526259	-0.060817	4.815474
299.748329	8000.280398	9.531264	-0.060850	4.815456
300.028347	8000.241213	9.536269	-0.060902	4.815443
299.964752	8000.223054	9.541274	-0.060890	4.815438
300.007988	8000.079465	9.546279	-0.060898	4.815396
300.056482	8000.199984	9.551283	-0.060907	4.815431
299.951590	8000.229241	9.556288	-0.060888	4.815440
300.120208	8000.296170	9.561293	-0.060919	4.815459
300.043908	8000.270316	9.566298	-0.060905	4.815452
300.018157	8000.353262	9.571303	-0.060900	4.815476
299.927086	8000.258753	9.576307	-0.060883	4.815449
300.096695	8000.401592	9.581312	-0.060915	4.815490
300.093668	8000.361989	9.586317	-0.060914	4.815478
300.020601	8000.392842	9.591322	-0.060900	4.815488
300.009288	8000.325310	9.596327	-0.060898	4.815468
300.338803	8000.223881	9.601331	-0.060960	4.815437
300.355037	8000.182459	9.606336	-0.060962	4.815424
300.284437	8000.122496	9.611341	-0.060949	4.815407
300.161990	8000.182459	9.616346	-0.060926	4.815425
300.268989	8000.197058	9.621351	-0.060946	4.815429
300.451191	8000.140218	9.626355	-0.060980	4.815412
300.356984	8000.410159	9.631360	-0.060963	4.815491
300.372077	8000.245792	9.636365	-0.060966	4.815443
300.352523	8000.212329	9.641370	-0.060962	4.815433
300.295471	8000.390959	9.646375	-0.060951	4.815486
300.447438	8000.192519	9.651379	-0.060979	4.815427
300.475091	8000.249628	9.656384	-0.060985	4.815444
300.210788	8000.150108	9.661389	-0.060935	4.815416
300.354335	8000.291446	9.666394	-0.060962	4.815456
300.593048	8000.159649	9.671399	-0.061006	4.815417
300.667335	8000.276323	9.676403	-0.061020	4.815450
300.590631	8000.208774	9.681408	-0.061006	4.815431
300.557926	8000.130198	9.686413	-0.061000	4.815408
300.661980	8000.424808	9.691418	-0.061019	4.815494
300.537250	8000.186503	9.696423	-0.060996	4.815425
300.761584	8000.098294	9.701427	-0.061038	4.815398
300.638317	8000.167864	9.706432	-0.061015	4.815419
300.746727	8000.086284	9.711437	-0.061035	4.815395
300.618591	8000.207082	9.716442	-0.061011	4.815430
300.700292	8000.256536	9.721447	-0.061026	4.815444
300.714902	8000.289913	9.726451	-0.061029	4.815454
300.466156	8000.266543	9.731456	-0.060982	4.815449
300.624591	8000.278789	9.736461	-0.061012	4.815451
300.552640	8000.387692	9.741466	-0.060999	4.815483
300.493420	8000.354639	9.746471	-0.060988	4.815474
300.780896	8000.145620	9.751475	-0.061041	4.815412
300.765818	8000.195607	9.756480	-0.061038	4.815426
300.801192	8000.157709	9.761485	-0.061045	4.815415
300.761889	8000.235086	9.766490	-0.061037	4.815438
300.758615	8000.310924	9.771495	-0.061037	4.815460
300.826274	8000.173082	9.776499	-0.061049	4.815419
300.841019	8000.227840	9.781504	-0.061052	4.815435
300.800541	8000.259233	9.786509	-0.061044	4.815445
300.807446	8000.084041	9.791514	-0.061046	4.815394
300.664737	8000.371351	9.796519	-0.061019	4.815478
300.710406	8000.161527	9.801523	-0.061027	4.815417
300.727939	8000.280466	9.806528	-0.061031	4.815451
300.760767	8000.146323	9.811533	-0.061037	4.815412
300.923008	8000.366005	9.816538	-0.061067	4.815475
301.076510	8000.215691	9.821543	-0.061096	4.815431
300.986599	7999.999342	9.826547	-0.061079	4.815368
300.868811	8000.180172	9.831552	-0.061057	4.815421
301.084579	8000.271402	9.836557	-0.061097	4.815447
301.184554	8000.286954	9.841562	-0.061116	4.815451
301.140589	8000.319360	9.846567	-0.061107	4.815461
301.164285	8000.211787	9.851571	-0.061112	4.815429
301.197204	8000.201641	9.856576	-0.061118	4.815426
301.312024	8000.084891	9.861581	-0.061139	4.815391
300.995694	8000.216464	9.866586	-0.061080	4.815431
301.245638	8000.214195	9.871591	-0.061127	4.815429
301.314072	8000.191811	9.876595	-0.061139	4.815423
301.152213	8000.201950	9.881600	-0.061109	4.815426
301.115829	8000.051693	9.886605	-0.061102	4.815383
301.327466	8000.133234	9.891610	-0.061142	4.815405
301.205464	8000.193205	9.896615	-0.061119	4.815424
301.251672	8000.181142	9.901619	-0.061128	4.815420
301.258098	8000.232555	9.906624	-0.061129	4.815435
301.415136	8000.067334	9.911629	-0.061158	4.815386
301.253903	8000.213239	9.916634	-0.061128	4.815429
301.354035	8000.355999	9.921639	-0.061147	4.815470
301.319122	8000.137352	9.926643	-0.061140	4.815407
301.122586	8000.324360	9.931648	-0.061104	4.815462
301.482388	8000.050265	9.936653	-0.061170	4.815380
301.584017	8000.169532	9.941658	-0.061189	4.815415
301.566349	8000.218408	9.946663	-0.061186	4.815429
301.551491	7999.950923	9.951667	-0.061183	4.815351
301.443658	8000.176815	9.956672	-0.061163	4.815418
301.462767	8000.219888	9.961677	-0.061167	4.815430
301.388597	8000.176965	9.966682	-0.061153	4.815418
301.396673	8000.258337	9.971687	-0.061154	4.815442
301.682761	8000.169014	9.976691	-0.061207	4.815414
301.329347	8000.259352	9.981696	-0.061142	4.815442
301.312387	8000.046349	9.986701	-0.061138	4.815380
301.624593	8000.204385	9.991706	-0.061197	4.815425
301.528129	8000.071301	9.996711	-0.061178	4.815386
301.440347	8000.092290	10.001715	-0.061162	4.815393
301.335725	8000.246617	10.006720	-0.061143	4.815439
301.420767	8000.067374	10.011725	-0.061158	4.815386
301.447477	8000.102021	10.016730	-0.061163	4.815396
301.632265	7999.957571	10.021735	-0.061198	4.815353
301.628258	8000.183048	10.026739	-0.061197	4.815419
301.513823	8000.184353	10.031744	-0.061176	4.815419
301.395402	8000.179179	10.036749	-0.061154	4.815419
301.613917	8000.226629	10.041754	-0.061194	4.815431
301.546554	8000.169923	10.046759	-0.061182	4.815415
301.669526	8000.216857	10.051763	-0.061205	4.815428
301.639542	8000.318976	10.056768	-0.061199	4.815458
301.802692	8000.129270	10.061773	-0.061229	4.815402
301.653718	8000.193070	10.066778	-0.061202	4.815421
301.208919	8000.202789	10.071783	-0.061119	4.815426
301.665586	8000.105608	10.076787	-0.061204	4.815396
301.478043	8000.126010	10.081792	-0.061169	4.815403
301.574586	8000.126540	10.086797	-0.061187	4.815402
301.691584	8000.061135	10.091802	-0.061208	4.815383
301.679283	8000.260822	10.096807	-0.061206	4.815441
301.651964	8000.230435	10.101811	-0.061201	4.815432
301.456375	8000.214359	10.106816	-0.061165	4.815429
301.642638	7999.970522	10.111821	-0.061199	4.815356
301.431638	8000.173324	10.116826	-0.061160	4.815417
301.448146	8000.218491	10.121831	-0.061163	4.815430
301.772769	8000.182186	10.126835	-0.061223	4.815418
301.622722	8000.238485	10.131840	-0.061195	4.815435
301.576185	8000.047438	10.136845	-0.061187	4.815379
301.674981	8000.294933	10.141850	-0.061205	4.815451
301.567162	8000.224728	10.146855	-0.061185	4.815431
301.702888	8000.235529	10.151859	-0.061210	4.815434
301.694636	8000.206528	10.156864	-0.061209	4.815425
301.812387	8000.038517	10.161869	-0.061230	4.815375
301.755645	8000.210742	10.166874	-0.061220	4.815426
301.637576	8000.187401	10.171879	-0.061198	4.815420
301.988497	8000.092740	10.176883	-0.061263	4.815390
301.881016	8000.128367	10.181888	-0.061243	4.815401
301.853296	8000.115077	10.186893	-0.061238	4.815398
301.819476	8000.167961	10.191898	-0.061232	4.815413
301.671722	8000.100301	10.196903	-0.061204	4.815394
301.606938	8000.040431	10.201907	-0.061192	4.815377
301.556775	8000.099457	10.206912	-0.061183	4.815395
301.818717	7999.947735	10.211917	-0.061231	4.815349
301.840617	7999.994060	10.216922	-0.061235	4.815362
301.816135	8000.103752	10.221927	-0.061231	4.815395
301.793991	7999.956937	10.226931	-0.061227	4.815352
301.910369	8000.211137	10.231936	-0.061248	4.815425
301.853365	8000.136431	10.236941	-0.061238	4.815404
301.688460	8000.238449	10.241946	-0.061207	4.815434
301.642844	8000.240896	10.246951	-0.061198	4.815435
301.703916	7999.941533	10.251955	-0.061210	4.815348
301.785231	8000.153461	10.256960	-0.061225	4.815409
301.845001	8000.024039	10.261965	-0.061236	4.815371
301.713336	8000.157608	10.266970	-0.061211	4.815411
301.769341	8000.138224	10.271975	-0.061222	4.815405
301.878144	8000.041684	10.276979	-0.061242	4.815376
301.806163	8000.278863	10.281984	-0.061229	4.815446
301.828318	8000.110334	10.286989	-0.061233	4.815396
301.735121	8000.196438	10.291994	-0.061215	4.815422
301.858864	8000.202765	10.296999	-0.061238	4.815423
301.857075	7999.944047	10.302003	-0.061238	4.815348
301.667309	8000.142926	10.307008	-0.061203	4.815407
301.786838	8000.140631	10.312013	-0.061225	4.815405
301.859100	8000.154655	10.317018	-0.061238	4.815409
301.651269	8000.125549	10.322023	-0.061200	4.815402
301.855208	8000.048759	10.327027	-0.061237	4.815378
301.818143	8000.197795	10.332032	-0.061231	4.815422
302.007318	7999.997831	10.337037	-0.061266	4.815363
301.870361	8000.131312	10.342042	-0.061240	4.815402
301.937983	8000.363327	10.347047	-0.061253	4.815470
302.051281	8000.180274	10.352051	-0.061274	4.815416
301.970306	8000.165031	10.357056	-0.061259	4.815412
302.028508	8000.251511	10.362061	-0.061270	4.815437
302.040042	8000.123425	10.367066	-0.061272	4.815399
301.914047	8000.306261	10.372071	-0.061248	4.815453
302.146585	7999.977672	10.377075	-0.061291	4.815356
301.931689	8000.185756	10.382080	-0.061251	4.815418
301.918490	8000.125673	10.387085	-0.061249	4.815400
301.937296	8000.180499	10.392090	-0.061252	4.815416
302.120441	8000.295777	10.397095	-0.061287	4.815449
302.089989	7999.947858	10.402099	-0.061281	4.815348
301.974638	8000.196076	10.407104	-0.061259	4.815421
301.970775	8000.065597	10.412109	-0.061258	4.815383
302.142518	8000.265133	10.417114	-0.061291	4.815440
302.029846	8000.129640	10.422119	-0.061269	4.815401
302.016759	8000.134765	10.427123	-0.061267	4.815403
302.001961	8000.216826	10.432128	-0.061264	4.815427
302.003447	8000.197607	10.437133	-0.061264	4.815421
301.984922	8000.124608	10.442138	-0.061261	4.815400
301.957237	8000.333662	10.447143	-0.061256	4.815461
301.890861	8000.136938	10.452147	-0.061243	4.815404
301.851106	8000.089242	10.457152	-0.061236	4.815390
301.726926	8000.112833	10.462157	-0.061213	4.815398
302.145173	8000.198874	10.467162	-0.061291	4.815421
302.014021	8000.313212	10.472167	-0.061266	4.815455
302.110934	8000.065750	10.477171	-0.061284	4.815382
302.123550	8000.189956	10.482176	-0.061287	4.815418
302.205194	8000.083343	10.487181	-0.061302	4.815387
302.022748	8000.024728	10.492186	-0.061268	4.815370
302.103741	8000.081654	10.497191	-0.061283	4.815387
302.329449	7999.952847	10.502195	-0.061325	4.815348
302.187235	8000.203827	10.507200	-0.061298	4.815422
301.877914	8000.091795	10.512205	-0.061241	4.815391
301.992525	8000.139659	10.517210	-0.061262	4.815404
301.855336	8000.144863	10.522215	-0.061236	4.815406
301.879265	8000.173050	10.527219	-0.061241	4.815414
301.924773	8000.218699	10.532224	-0.061249	4.815428
302.089660	8000.348640	10.537229	-0.061280	4.815465
302.116134	8000.203697	10.542234	-0.061285	4.815422
301.984993	8000.314828	10.547239	-0.061260	4.815455
302.176697	7999.960975	10.552243	-0.061296	4.815351
302.040773	8000.143646	10.557248	-0.061271	4.815405
302.159864	8000.243964	10.562253	-0.061293	4.815434
302.096382	8000.350873	10.567258	-0.061281	4.815465
302.315530	8000.307474	10.572263	-0.061322	4.815452
302.328845	7999.999831	10.577267	-0.061324	4.815362
302.222033	8000.113503	10.582272	-0.061304	4.815395
302.524962	8000.092873	10.587277	-0.061361	4.815388
302.315287	8000.164217	10.592282	-0.061322	4.815410
302.295722	8000.223752	10.597287	-0.061318	4.815427
302.265071	8000.164448	10.602291	-0.061312	4.815410
302.197993	8000.355746	10.607296	-0.061300	4.815466
302.446825	8000.154631	10.612301	-0.061346	4.815406
302.536254	8000.047079	10.617306	-0.061362	4.815375
302.469897	8000.069492	10.622311	-0.061350	4.815381
302.535165	8000.045986	10.627315	-0.061362	4.815374
302.141992	8000.245768	10.632320	-0.061289	4.815434
302.358284	8000.112528	10.637325	-0.061329	4.815395
302.419678	8000.155234	10.642330	-0.061341	4.815407
302.304372	8000.285869	10.647335	-0.061319	4.815445
302.309532	8000.107435	10.652339	-0.061320	4.815393
302.172568	8000.123331	10.657344	-0.061295	4.815399
302.266188	8000.105641	10.662349	-0.061312	4.815393
302.466781	7999.996727	10.667354	-0.061349	4.815360
302.174174	8000.176798	10.672359	-0.061295	4.815414
302.221815	8000.144448	10.677363	-0.061304	4.815404
302.335756	8000.181612	10.682368	-0.061325	4.815415
302.408875	7999.943377	10.687373	-0.061338	4.815345
302.335573	8000.101432	10.692378	-0.061325	4.815391
302.316094	8000.091485	10.697383	-0.061321	4.815389
302.497200	8000.056006	10.702387	-0.061355	4.815377
302.276541	8000.159237	10.707392	-0.061314	4.815409
302.342078	8000.006392	10.712397	-0.061326	4.815364
302.305848	8000.163994	10.717402	-0.061319	4.815410
302.173112	8000.191719	10.722407	-0.061294	4.815419
302.448620	7999.966463	10.727411	-0.061345	4.815351
302.399782	8000.260683	10.732416	-0.061337	4.815438
302.333052	8000.120607	10.737421	-0.061324	4.815397
302.541197	8000.084508	10.742426	-0.061363	4.815385
302.395670	8000.248848	10.747431	-0.061336	4.815434
302.596663	8000.033044	10.752435	-0.061373	4.815370
302.454194	8000.199573	10.757440	-0.061346	4.815419
302.093688	8000.272689	10.762445	-0.061279	4.815443
302.309109	8000.231366	10.767450	-0.061319	4.815429
302.217566	8000.301465	10.772455	-0.061302	4.815450
302.269293	8000.037218	10.777459	-0.061312	4.815373
301.999841	8000.196294	10.782464	-0.061262	4.815421
302.196642	8000.062731	10.787469	-0.061298	4.815381
302.324958	8000.207030	10.792474	-0.061322	4.815422
302.154582	8000.277957	10.797479	-0.061290	4.815444
302.315284	8000.136312	10.802483	-0.061320	4.815402
302.178942	8000.356391	10.807488	-0.061295	4.815467
302.244748	8000.380999	10.812493	-0.061307	4.815473
302.541173	8000.399815	10.817498	-0.061362	4.815478
302.469981	8000.276766	10.822503	-0.061349	4.815442
302.706096	8000.123544	10.827507	-0.061393	4.815396
302.552209	8000.184056	10.832512	-0.061364	4.815414
302.594985	8000.164453	10.837517	-0.061372	4.815409
302.685615	8000.110369	10.842522	-0.061389	4.815392
302.544051	8000.182844	10.847527	-0.061363	4.815414
302.499719	8000.103002	10.852531	-0.061354	4.815391
302.395938	8000.248794	10.857536	-0.061335	4.815434
302.585158	8000.223070	10.862541	-0.061370	4.815426
302.640175	8000.246430	10.867546	-0.061380	4.815432
302.496707	8000.256873	10.872551	-0.061354	4.815436
302.560260	8000.124304	10.877555	-0.061365	4.815397
302.303498	8000.138212	10.882560	-0.061318	4.815402
302.356719	8000.068541	10.887565	-0.061327	4.815382
302.430466	8000.084728	10.892570	-0.061341	4.815386
302.500049	8000.175673	10.897575	-0.061354	4.815412
302.644524	8000.029482	10.902579	-0.061381	4.815369
302.524169	8000.225241	10.907584	-0.061359	4.815427
302.391778	8000.117213	10.912589	-0.061334	4.815396
302.532103	8000.071436	10.917594	-0.061360	4.815382
302.418544	8000.151858	10.922599	-0.061339	4.815406
302.607524	7999.977545	10.927603	-0.061374	4.815354
302.517018	8000.035902	10.932608	-0.061357	4.815371
302.454333	8000.049824	10.937613	-0.061345	4.815376
302.351634	8000.208461	10.942618	-0.061326	4.815423
302.503617	8000.245189	10.947623	-0.061355	4.815433
302.585123	8000.035952	10.952627	-0.061370	4.815371
302.691198	8000.172400	10.957632	-0.061389	4.815410
302.708420	8000.103200	10.962637	-0.061392	4.815390
302.589247	7999.998599	10.967642	-0.061370	4.815360
302.511611	8000.122376	10.972647	-0.061356	4.815397
302.534043	8000.054332	10.977651	-0.061360	4.815377
302.700210	8000.095571	10.982656	-0.061391	4.815388
302.492346	8000.031187	10.987661	-0.061352	4.815370
302.634097	7999.944813	10.992666	-0.061378	4.815344
302.446704	8000.191837	10.997671	-0.061344	4.815417
302.529373	8000.091655	11.002675	-0.061359	4.815388
302.631799	8000.088008	11.007680	-0.061378	4.815386
302.650811	8000.084045	11.012685	-0.061381	4.815385
302.479454	8000.120750	11.017690	-0.061350	4.815396
302.684964	7999.939227	11.022695	-0.061388	4.815342
302.702827	7999.971590	11.027699	-0.061391	4.815352
302.643880	8000.084988	11.032704	-0.061380	4.815385
302.689126	8000.093219	11.037709	-0.061388	4.815387
302.856318	7999.946336	11.042714	-0.061419	4.815344
302.662211	8000.285182	11.047719	-0.061384	4.815444
302.605083	7999.998816	11.052723	-0.061373	4.815360
302.586982	8000.291411	11.057728	-0.061369	4.815446
302.548715	8000.042772	11.062733	-0.061362	4.815373
302.493257	8000.192573	11.067738	-0.061352	4.815417
302.486375	8000.296146	11.072743	-0.061351	4.815448
302.587592	8000.098995	11.077747	-0.061369	4.815390
302.445351	8000.095563	11.082752	-0.061343	4.815389
302.339591	8000.193218	11.087757	-0.061323	4.815418
302.657508	8000.179252	11.092762	-0.061382	4.815413
302.613101	8000.135753	11.097767	-0.061374	4.815400
302.433627	8000.208668	11.102771	-0.061341	4.815422
302.430479	8000.105992	11.107776	-0.061340	4.815392
302.521532	8000.095742	11.112781	-0.061357	4.815389
302.565475	8000.116779	11.117786	-0.061365	4.815395
302.344165	8000.293759	11.122791	-0.061324	4.815448
302.765507	8000.034577	11.127795	-0.061402	4.815370
302.456695	8000.113897	11.132800	-0.061345	4.815395
302.501889	8000.092196	11.137805	-0.061353	4.815388
302.670866	8000.026584	11.142810	-0.061384	4.815368
302.413381	8000.216859	11.147815	-0.061337	4.815425
302.509202	8000.378794	11.152819	-0.061354	4.815472
302.496987	8000.269553	11.157824	-0.061352	4.815440
302.661911	8000.224184	11.162829	-0.061383	4.815426
302.694810	8000.032313	11.167834	-0.061389	4.815370
302.599027	8000.108755	11.172839	-0.061371	4.815392
302.766201	8000.057010	11.177843	-0.061402	4.815376
302.628937	8000.233247	11.182848	-0.061376	4.815429
302.680915	8000.144313	11.187853	-0.061386	4.815402
302.734394	8000.240337	11.192858	-0.061396	4.815430
302.567274	8000.144559	11.197863	-0.061365	4.815403
302.615072	8000.097247	11.202867	-0.061374	4.815389
302.659910	8000.251920	11.207872	-0.061382	4.815434
302.668323	8000.162263	11.212877	-0.061384	4.815408
302.517418	8000.089204	11.217882	-0.061355	4.815387
302.558970	8000.261995	11.222887	-0.061363	4.815437
302.841402	8000.102059	11.227891	-0.061416	4.815389
302.719924	8000.221903	11.232896	-0.061393	4.815425
302.437417	8000.195831	11.237901	-0.061340	4.815419
302.550505	8000.102567	11.242906	-0.061361	4.815391
302.687646	8000.270532	11.247911	-0.061387	4.815439
302.635720	8000.182011	11.252915	-0.061377	4.815414
302.594584	8000.214464	11.257920	-0.061370	4.815423
302.805539	8000.093962	11.262925	-0.061409	4.815387
302.792972	8000.040303	11.267930	-0.061406	4.815371
302.768101	8000.276130	11.272935	-0.061402	4.815440
302.958342	8000.018456	11.277939	-0.061437	4.815364
302.509542	8000.250453	11.282944	-0.061354	4.815434
302.380684	8000.308173	11.287949	-0.061330	4.815452
302.488581	8000.230858	11.292954	-0.061350	4.815429
302.666573	8000.194258	11.297959	-0.061383	4.815417
302.807059	8000.124966	11.302963	-0.061409	4.815396
302.788007	8000.150303	11.307968	-0.061405	4.815404
302.605887	8000.268071	11.312973	-0.061371	4.815439
302.713504	8000.188613	11.317978	-0.061391	4.815415
302.674265	8000.367547	11.322983	-0.061384	4.815468
302.810275	8000.192352	11.327987	-0.061409	4.815416
302.829915	8000.203365	11.332992	-0.061413	4.815419
302.692835	8000.147638	11.337997	-0.061387	4.815403
302.712093	8000.028230	11.343002	-0.061391	4.815368
302.713950	8000.195018	11.348007	-0.061391	4.815417
302.793188	8000.147158	11.353011	-0.061406	4.815403
302.768548	8000.114677	11.358016	-0.061401	4.815393
302.916399	8000.111784	11.363021	-0.061429	4.815392
303.003043	8000.013805	11.368026	-0.061445	4.815363
302.815998	8000.318563	11.373031	-0.061410	4.815453
303.002729	7999.971036	11.378035	-0.061445	4.815350
302.891868	8000.283472	11.383040	-0.061424	4.815442
302.902340	8000.264401	11.388045	-0.061426	4.815436
303.083176	8000.118812	11.393050	-0.061460	4.815393
302.830826	8000.107138	11.398055	-0.061413	4.815391
302.701919	8000.021616	11.403059	-0.061389	4.815366
302.586728	8000.261288	11.408064	-0.061367	4.815437
302.781820	8000.017592	11.413069	-0.061403	4.815365
302.781577	8000.170448	11.418074	-0.061403	4.815409
302.676752	8000.150532	11.423079	-0.061384	4.815404
302.567470	8000.004405	11.428083	-0.061363	4.815362
302.795345	8000.266876	11.433088	-0.061406	4.815438
302.625452	8000.244811	11.438093	-0.061374	4.815432
302.613356	8000.168711	11.443098	-0.061372	4.815410
302.646668	8000.136123	11.448103	-0.061378	4.815400
303.060577	8000.046784	11.453107	-0.061455	4.815372
302.948938	8000.020342	11.458112	-0.061434	4.815365
302.789025	8000.140616	11.463117	-0.061405	4.815401
303.042363	7999.976990	11.468122	-0.061452	4.815352
302.809403	8000.174087	11.473127	-0.061408	4.815410
303.009135	8000.011709	11.478131	-0.061445	4.815362
302.868724	8000.031824	11.483136	-0.061419	4.815369
302.732890	8000.136464	11.488141	-0.061394	4.815400
302.979649	7999.958832	11.493146	-0.061440	4.815347
302.702303	8000.202227	11.498151	-0.061388	4.815419
302.795849	8000.220881	11.503155	-0.061406	4.815424
302.707655	8000.105034	11.508160	-0.061389	4.815391
302.724612	8000.134175	11.513165	-0.061392	4.815399
302.860873	8000.111848	11.518170	-0.061418	4.815392
302.691735	8000.188142	11.523175	-0.061386	4.815415
302.875697	8000.055433	11.528179	-0.061420	4.815375
303.026508	8000.052589	11.533184	-0.061448	4.815374
303.050112	8000.158807	11.538189	-0.061453	4.815405
303.096289	8000.028087	11.543194	-0.061461	4.815366
303.032650	8000.194857	11.548199	-0.061449	4.815415
303.108340	7999.978040	11.553203	-0.061463	4.815352
302.761805	8000.094148	11.558208	-0.061399	4.815387
302.844385	8000.079481	11.563213	-0.061414	4.815383
302.913507	7999.980143	11.568218	-0.061427	4.815353
302.830104	8000.030066	11.573223	-0.061411	4.815368
303.096788	7999.938283	11.578227	-0.061461	4.815340
302.924746	8000.088287	11.583232	-0.061429	4.815385
302.843218	8000.148932	11.588237	-0.061414	4.815403
302.868760	8000.098042	11.593242	-0.061419	4.815388
303.030469	8000.072931	11.598247	-0.061449	4.815380
302.841707	8000.105071	11.603251	-0.061413	4.815390
302.793647	8000.251789	11.608256	-0.061405	4.815433
302.885976	8000.109007	11.613261	-0.061422	4.815391
302.919388	8000.032593	11.618266	-0.061428	4.815369
302.830034	8000.061038	11.623271	-0.061411	4.815377
302.894097	7999.917789	11.628275	-0.061423	4.815335
302.931166	8000.106540	11.633280	-0.061430	4.815390
302.999637	8000.065984	11.638285	-0.061443	4.815378
302.906713	7999.946852	11.643290	-0.061425	4.815344
302.835128	8000.078213	11.648295	-0.061412	4.815382
303.033540	8000.098608	11.653299	-0.061449	4.815387
302.877852	8000.186883	11.658304	-0.061420	4.815414
302.771358	8000.134871	11.663309	-0.061400	4.815399
303.101472	8000.019554	11.668314	-0.061461	4.815364
302.837966	8000.141316	11.673319	-0.061412	4.815401
302.741704	7999.972957	11.678323	-0.061394	4.815352
302.709033	8000.116722	11.683328	-0.061388	4.815394
302.859339	8000.063628	11.688333	-0.061416	4.815378
302.807529	8000.054214	11.693338	-0.061407	4.815375
302.759384	8000.165654	11.698343	-0.061398	4.815408
303.023361	8000.053515	11.703347	-0.061447	4.815374
302.960444	8000.103779	11.708352	-0.061435	4.815389
302.760503	7999.998905	11.713357	-0.061398	4.815360
303.128168	8000.098006	11.718362	-0.061466	4.815387
302.943548	8000.218940	11.723367	-0.061432	4.815423
302.913646	7999.923405	11.728371	-0.061426	4.815337
303.019032	8000.069462	11.733376	-0.061446	4.815379
302.984946	7999.951307	11.738381	-0.061439	4.815345
302.847410	8000.175643	11.743386	-0.061414	4.815411
302.889699	8000.235136	11.748391	-0.061422	4.815428
303.016488	7999.977477	11.753395	-0.061445	4.815352
302.943100	8000.175086	11.758400	-0.061431	4.815410
302.811812	8000.080972	11.763405	-0.061407	4.815383
303.010774	8000.191169	11.768410	-0.061444	4.815414
302.929552	8000.141714	11.773415	-0.061429	4.815400
302.873226	8000.150397	11.778419	-0.061418	4.815403
302.917648	8000.086994	11.783424	-0.061427	4.815385
302.927798	8000.346922	11.788429	-0.061429	4.815460
302.872646	8000.117241	11.793434	-0.061418	4.815394
302.839399	8000.178687	11.798439	-0.061412	4.815412
302.907918	8000.019476	11.803443	-0.061425	4.815365
302.828729	8000.145367	11.808448	-0.061410	4.815402
302.666650	8000.143742	11.813453	-0.061380	4.815402
302.764757	7999.921954	11.818458	-0.061398	4.815337
302.847296	8000.270737	11.823463	-0.061413	4.815439
302.933876	8000.048756	11.828467	-0.061429	4.815373
303.019839	8000.055525	11.833472	-0.061445	4.815375
303.098797	8000.125248	11.838477	-0.061460	4.815395
303.145498	8000.002019	11.843482	-0.061469	4.815359
302.998283	8000.072263	11.848487	-0.061441	4.815380
302.816687	8000.002970	11.853491	-0.061407	4.815360
303.159398	8000.158313	11.858496	-0.061471	4.815404
302.888388	7999.998810	11.863501	-0.061421	4.815359
303.046872	8000.176750	11.868506	-0.061450	4.815410
303.028699	8000.167893	11.873511	-0.061447	4.815408
302.888175	7999.808523	11.878515	-0.061420	4.815303
302.814596	8000.135471	11.883520	-0.061407	4.815399
302.985893	8000.073105	11.888525	-0.061439	4.815380
302.913205	8000.213000	11.893530	-0.061425	4.815421
302.703185	8000.105820	11.898535	-0.061386	4.815391
302.938623	7999.914105	11.903539	-0.061430	4.815334
302.902480	8000.174331	11.908544	-0.061423	4.815410
302.988458	8000.169342	11.913549	-0.061439	4.815408
302.996272	7999.943916	11.918554	-0.061440	4.815342
303.110617	8000.179917	11.923559	-0.061462	4.815411
303.124221	7999.992000	11.928563	-0.061464	4.815356
303.137245	8000.044593	11.933568	-0.061466	4.815371
303.232335	8000.063273	11.938573	-0.061484	4.815376
303.176196	7999.928716	11.943578	-0.061474	4.815337
303.067445	8000.109703	11.948583	-0.061453	4.815390
303.013533	8000.139805	11.953587	-0.061443	4.815399
303.065698	8000.147083	11.958592	-0.061453	4.815401
303.214545	8000.211552	11.963597	-0.061481	4.815419
303.117321	8000.190694	11.968602	-0.061463	4.815414
302.978414	8000.095384	11.973607	-0.061437	4.815387
303.054483	8000.159713	11.978611	-0.061451	4.815405
302.870779	8000.160937	11.983616	-0.061417	4.815406
302.968662	8000.190353	11.988621	-0.061435	4.815414
303.233924	8000.100684	11.993626	-0.061484	4.815387
303.199172	8000.195244	11.998631	-0.061478	4.815415
302.992992	8000.098816	12.003635	-0.061439	4.815388
303.059008	8000.003702	12.008640	-0.061451	4.815360
303.104703	7999.958492	12.013645	-0.061460	4.815346
303.058364	8000.040031	12.018650	-0.061451	4.815370
302.996054	8000.111684	12.023655	-0.061440	4.815391
303.091215	7999.908019	12.028659	-0.061457	4.815331
302.893097	8000.038349	12.033664	-0.061420	4.815370
303.163699	8000.114460	12.038669	-0.061471	4.815391
303.128441	7999.926801	12.043674	-0.061464	4.815337
302.933964	8000.057192	12.048679	-0.061428	4.815376
303.028576	7999.935828	12.053683	-0.061445	4.815340
303.071187	8000.030602	12.058688	-0.061453	4.815367
302.838151	8000.054524	12.063693	-0.061410	4.815375
303.099326	7999.994719	12.068698	-0.061459	4.815357
302.974259	8000.174365	12.073703	-0.061435	4.815410
303.084110	8000.077841	12.078707	-0.061456	4.815381
302.898551	8000.107896	12.083712	-0.061421	4.815391
303.236344	8000.096397	12.088717	-0.061484	4.815386
303.415245	8000.151745	12.093722	-0.061517	4.815401
303.196918	8000.142772	12.098727	-0.061477	4.815399
303.000116	7999.986639	12.103731	-0.061440	4.815355
303.121755	8000.129760	12.108736	-0.061463	4.815396
303.205776	8000.257293	12.113741	-0.061478	4.815433
303.231464	7999.977644	12.118746	-0.061483	4.815351
303.030067	8000.191300	12.123751	-0.061445	4.815414
302.947933	8000.200623	12.128755	-0.061430	4.815418
303.045448	7999.960651	12.133760	-0.061448	4.815347
302.895386	7999.983813	12.138765	-0.061420	4.815355
303.035097	7999.971164	12.143770	-0.061446	4.815350
302.961424	8000.055456	12.148775	-0.061432	4.815375
303.110174	7999.968129	12.153779	-0.061460	4.815349
303.199950	7999.940754	12.158784	-0.061477	4.815340
302.973947	8000.118725	12.163789	-0.061435	4.815394
303.109298	7999.967037	12.168794	-0.061460	4.815349
303.145469	8000.105533	12.173799	-0.061467	4.815389
303.232330	7999.953040	12.178803	-0.061483	4.815344
303.219786	8000.214729	12.183808	-0.061480	4.815420
303.109976	8000.002314	12.188813	-0.061460	4.815359
303.048156	7999.963871	12.193818	-0.061448	4.815348
302.962298	8000.243584	12.198823	-0.061432	4.815430
303.126634	8000.141549	12.203827	-0.061463	4.815399
303.015795	8000.021050	12.208832	-0.061442	4.815365
302.918793	8000.116714	12.213837	-0.061424	4.815393
302.989558	8000.049472	12.218842	-0.061437	4.815373
303.013678	7999.985731	12.223847	-0.061442	4.815355
303.202695	8000.159903	12.228851	-0.061477	4.815404
303.074702	8000.097912	12.233856	-0.061453	4.815387
302.983092	8000.209700	12.238861	-0.061436	4.815420
303.169830	8000.092003	12.243866	-0.061471	4.815385
303.127882	8000.176822	12.248871	-0.061463	4.815410
303.225813	7999.922960	12.253875	-0.061481	4.815335
303.146665	8000.052058	12.258880	-0.061466	4.815373
303.156189	8000.161250	12.263885	-0.061468	4.815405
303.059400	8000.053811	12.268890	-0.061450	4.815374
303.168708	8000.149693	12.273895	-0.061470	4.815402
303.019199	8000.022138	12.278899	-0.061442	4.815365
303.280988	7999.996550	12.283904	-0.061491	4.815356
302.997774	8000.135089	12.288909	-0.061438	4.815398
303.268511	8000.038028	12.293914	-0.061489	4.815369
303.147590	8000.028535	12.298919	-0.061466	4.815366
303.046470	7999.930646	12.303923	-0.061447	4.815338
303.034480	7999.936859	12.308928	-0.061445	4.815340
303.012168	8000.219764	12.313933	-0.061441	4.815423
303.101439	8000.089759	12.318938	-0.061458	4.815385
302.981009	8000.209620	12.323943	-0.061435	4.815420
303.229789	8000.135712	12.328947	-0.061481	4.815397
303.063604	8000.027122	12.333952	-0.061450	4.815366
303.022352	7999.980469	12.338957	-0.061443	4.815353
303.167995	8000.061988	12.343962	-0.061470	4.815376
302.962088	8000.104533	12.348967	-0.061431	4.815390
303.028998	8000.023330	12.353971	-0.061444	4.815365
303.307022	8000.067495	12.358976	-0.061496	4.815377
303.176247	8000.066390	12.363981	-0.061471	4.815377
303.168126	7999.947596	12.368986	-0.061470	4.815343
303.154515	8000.012575	12.373991	-0.061467	4.815362
303.006990	8000.014399	12.378995	-0.061440	4.815363
303.092755	7999.988027	12.384000	-0.061455	4.815355
303.307359	7999.955242	12.389005	-0.061495	4.815344
303.236291	7999.969025	12.394010	-0.061482	4.815349
303.182086	8000.082503	12.399015	-0.061472	4.815382
303.228096	8000.067229	12.404019	-0.061481	4.815377
303.290927	7999.998786	12.409024	-0.061492	4.815357
303.181102	7999.977719	12.414029	-0.061472	4.815351
303.112721	7999.934891	12.419034	-0.061459	4.815339
303.160441	8000.112062	12.424039	-0.061468	4.815391
303.241692	8000.027890	12.429043	-0.061483	4.815366
303.266295	7999.998364	12.434048	-0.061487	4.815357
303.114982	8000.139092	12.439053	-0.061459	4.815399
303.372343	7999.836566	12.444058	-0.061507	4.815309
303.245027	8000.127349	12.449063	-0.061484	4.815395
303.141408	7999.957797	12.454067	-0.061464	4.815346
303.136389	7999.963056	12.459072	-0.061463	4.815347
303.276404	7999.908722	12.464077	-0.061489	4.815331
303.323094	7999.908425	12.469082	-0.061498	4.815331
302.921209	8000.089891	12.474087	-0.061423	4.815385
303.058690	7999.913652	12.479091	-0.061449	4.815333
303.147879	8000.054096	12.484096	-0.061465	4.815374
303.063331	8000.079414	12.489101	-0.061449	4.815382
303.212821	8000.147101	12.494106	-0.061477	4.815401
302.981941	8000.131507	12.499111	-0.061434	4.815397
303.270746	7999.977021	12.504115	-0.061488	4.815351
303.049746	8000.035350	12.509120	-0.061447	4.815369
303.213043	8000.103266	12.514125	-0.061477	4.815388
303.272304	7999.999487	12.519130	-0.061488	4.815357
303.211089	8000.199437	12.524135	-0.061477	4.815416
303.323395	8000.202368	12.529139	-0.061498	4.815416
303.365800	8000.108998	12.534144	-0.061505	4.815389
303.230771	8000.081098	12.539149	-0.061480	4.815381
303.147607	8000.114991	12.544154	-0.061465	4.815392
303.243701	8000.041755	12.549159	-0.061483	4.815370
303.237904	8000.194521	12.554163	-0.061482	4.815414
303.193898	8000.089027	12.559168	-0.061473	4.815384
302.845289	8000.168755	12.564173	-0.061408	4.815409
303.003088	8000.213063	12.569178	-0.061438	4.815421
302.998807	8000.142436	12.574183	-0.061437	4.815400
303.104208	7999.969941	12.579187	-0.061456	4.815350
303.374480	8000.057805	12.584192	-0.061507	4.815374
303.231513	8000.201879	12.589197	-0.061480	4.815417
303.203924	8000.091313	12.594202	-0.061475	4.815385
303.111985	8000.140026	12.599207	-0.061458	4.815399
303.200613	8000.089115	12.604211	-0.061474	4.815384
303.216604	7999.960032	12.609216	-0.061477	4.815346
303.162657	7999.992271	12.614221	-0.061467	4.815356
303.477255	8000.125769	12.619226	-0.061526	4.815393
303.194771	8000.242941	12.624231	-0.061473	4.815429
303.007217	7999.967235	12.629235	-0.061438	4.815349
303.142153	8000.293373	12.634240	-0.061463	4.815444
303.141502	8000.091322	12.639245	-0.061463	4.815385
303.253744	8000.075010	12.644250	-0.061484	4.815380
303.078338	8000.258098	12.649255	-0.061451	4.815434
303.296258	8000.078917	12.654259	-0.061492	4.815380
303.371773	8000.286483	12.659264	-0.061506	4.815441
303.189503	8000.237487	12.664269	-0.061472	4.815427
303.437325	8000.063079	12.669274	-0.061518	4.815375
303.358315	8000.182559	12.674279	-0.061503	4.815410
303.264883	8000.074107	12.679283	-0.061486	4.815379
303.492125	8000.113154	12.684288	-0.061528	4.815390
303.297109	8000.240329	12.689293	-0.061492	4.815428
303.206243	8000.072056	12.694298	-0.061475	4.815379
303.266189	8000.184223	12.699303	-0.061486	4.815411
303.439231	8000.132576	12.704307	-0.061518	4.815395
303.435095	8000.102573	12.709312	-0.061517	4.815387
303.298318	8000.214680	12.714317	-0.061492	4.815420
303.375071	8000.113329	12.719322	-0.061506	4.815390
303.491580	8000.060743	12.724327	-0.061528	4.815374
303.233923	8000.292708	12.729331	-0.061480	4.815443
303.343628	8000.103178	12.734336	-0.061500	4.815387
303.303360	8000.201923	12.739341	-0.061493	4.815416
303.349208	8000.150301	12.744346	-0.061501	4.815401
303.246610	8000.182802	12.749351	-0.061482	4.815411
303.339216	8000.185406	12.754355	-0.061499	4.815411
303.441863	8000.156108	12.759360	-0.061518	4.815402
303.210216	8000.195018	12.764365	-0.061475	4.815415
303.510237	7999.972303	12.769370	-0.061531	4.815348
303.446781	8000.139077	12.774375	-0.061519	4.815397
303.379115	8000.258747	12.779379	-0.061507	4.815433
303.496529	8000.201900	12.784384	-0.061528	4.815415
303.269556	8000.252646	12.789389	-0.061486	4.815431
303.316430	8000.095212	12.794394	-0.061495	4.815385
303.237518	8000.156969	12.799399	-0.061480	4.815404
303.281753	8000.064699	12.804403	-0.061488	4.815376
303.365489	8000.131295	12.809408	-0.061504	4.815395
303.184600	8000.174255	12.814413	-0.061470	4.815409
303.357334	7999.903462	12.819418	-0.061502	4.815329
303.339532	8000.058165	12.824423	-0.061499	4.815374
303.212474	8000.260229	12.829427	-0.061475	4.815434
303.528378	7999.998225	12.834432	-0.061534	4.815356
303.352560	8000.231549	12.839437	-0.061501	4.815425
303.482129	7999.972865	12.844442	-0.061525	4.815349
303.192344	8000.229952	12.849447	-0.061471	4.815425
303.285961	8000.303127	12.854451	-0.061489	4.815446
303.372492	8000.147419	12.859456	-0.061505	4.815400
303.352553	8000.209087	12.864461	-0.061501	4.815418
303.406821	7999.802704	12.869466	-0.061511	4.815299
303.359802	8000.131166	12.874471	-0.061502	4.815395
303.275003	8000.018581	12.879475	-0.061486	4.815363
303.296728	8000.145079	12.884480	-0.061491	4.815400
303.171654	8000.229587	12.889485	-0.061467	4.815425
303.367456	8000.067143	12.894490	-0.061504	4.815377
303.331383	8000.292098	12.899495	-0.061497	4.815443
303.491326	8000.172886	12.904499	-0.061527	4.815407
303.320429	8000.167908	12.909504	-0.061495	4.815406
303.190430	8000.237369	12.914509	-0.061471	4.815427
303.415730	8000.060448	12.919514	-0.061512	4.815375
303.386341	8000.127304	12.924519	-0.061507	4.815394
303.445362	8000.091936	12.929523	-0.061518	4.815384
303.564921	8000.096056	12.934528	-0.061540	4.815384
303.544405	8000.023022	12.939533	-0.061536	4.815363
303.360706	8000.045625	12.944538	-0.061502	4.815370
303.214004	8000.104118	12.949543	-0.061475	4.815388
303.250137	8000.253305	12.954547	-0.061482	4.815432
303.293560	8000.183470	12.959552	-0.061490	4.815411
303.286495	8000.294525	12.964557	-0.061488	4.815444
303.477069	8000.158718	12.969562	-0.061524	4.815403
303.477301	8000.250652	12.974567	-0.061524	4.815430
303.358914	8000.123612	12.979571	-0.061502	4.815393
303.399807	7999.990666	12.984576	-0.061509	4.815354
303.372608	8000.352598	12.989581	-0.061504	4.815460
303.356620	8000.063703	12.994586	-0.061501	4.815376
303.274344	8000.188474	12.999591	-0.061486	4.815413
303.313112	8000.138873	13.004595	-0.061493	4.815398
303.611748	7999.974929	13.009600	-0.061548	4.815349
303.300474	8000.316110	13.014605	-0.061491	4.815450
303.568811	8000.111041	13.019610	-0.061540	4.815389
303.563699	8000.120574	13.024615	-0.061539	4.815391
303.229058	8000.236880	13.029619	-0.061477	4.815427
303.393091	8000.101701	13.034624	-0.061508	4.815387
303.570515	8000.302409	13.039629	-0.061541	4.815444
303.616266	8000.151368	13.044634	-0.061549	4.815400
303.467027	8000.320996	13.049639	-0.061521	4.815450
303.518298	8000.217083	13.054643	-0.061531	4.815420
303.465889	8000.206589	13.059648	-0.061521	4.815417
303.347872	8000.160798	13.064653	-0.061499	4.815404
303.320003	8000.100469	13.069658	-0.061494	4.815387
303.453442	8000.143304	13.074663	-0.061519	4.815399
303.342633	8000.051666	13.079667	-0.061498	4.815372
303.383167	7999.953991	13.084672	-0.061505	4.815344
303.321066	8000.100476	13.089677	-0.061494	4.815387
303.447316	7999.921912	13.094682	-0.061517	4.815334
303.272382	8000.217251	13.099687	-0.061485	4.815421
303.451272	8000.126148	13.104691	-0.061518	4.815394
303.569525	8000.046865	13.109696	-0.061540	4.815370
303.505664	8000.052216	13.114701	-0.061528	4.815372
303.386608	7999.996788	13.119706	-0.061506	4.815356
303.431947	8000.105505	13.124711	-0.061514	4.815388
303.539930	8000.190677	13.129715	-0.061534	4.815412
303.508711	7999.979566	13.134720	-0.061528	4.815350
303.554526	8000.177017	13.139725	-0.061537	4.815408
303.565012	8000.116256	13.144730	-0.061539	4.815390
303.405219	8000.224775	13.149735	-0.061509	4.815423
303.286458	8000.219593	13.154739	-0.061487	4.815422
303.701592	8000.057583	13.159744	-0.061564	4.815372
303.403094	8000.146695	13.164749	-0.061509	4.815400
303.481599	8000.143720	13.169754	-0.061523	4.815399
303.711337	8000.135774	13.174759	-0.061566	4.815395
303.579998	7999.974311	13.179763	-0.061541	4.815349
303.429984	8000.020991	13.184768	-0.061513	4.815363
303.553026	8000.070066	13.189773	-0.061536	4.815377
303.564860	8000.028570	13.194778	-0.061539	4.815365
303.469609	8000.050503	13.199783	-0.061521	4.815371
303.488205	8000.105328	13.204787	-0.061524	4.815387
303.639753	8000.004150	13.209792	-0.061552	4.815357
303.577121	8000.160248	13.214797	-0.061541	4.815403
303.624346	7999.917301	13.219802	-0.061549	4.815332
303.711192	7999.873843	13.224807	-0.061566	4.815319
303.614100	8000.099922	13.229811	-0.061548	4.815385
303.409401	7999.909449	13.234816	-0.061509	4.815331
303.451133	8000.015968	13.239821	-0.061517	4.815361
303.626184	7999.936560	13.244826	-0.061550	4.815337
303.458630	8000.047087	13.249831	-0.061518	4.815370
303.241432	8000.156791	13.254835	-0.061478	4.815404
303.484954	8000.222833	13.259840	-0.061523	4.815422
303.430790	8000.294623	13.264845	-0.061513	4.815443
303.395795	8000.009688	13.269850	-0.061507	4.815360
303.521443	8000.295054	13.274855	-0.061530	4.815443
303.731575	8000.140330	13.279859	-0.061569	4.815396
303.606306	8000.070900	13.284864	-0.061546	4.815377
303.472313	8000.218331	13.289869	-0.061521	4.815420
303.790664	8000.132751	13.294874	-0.061580	4.815394
303.604947	7999.990696	13.299879	-0.061545	4.815353
303.468537	8000.110293	13.304883	-0.061520	4.815389
303.718309	8000.052436	13.309888	-0.061566	4.815371
303.643521	8000.126021	13.314893	-0.061553	4.815393
303.544418	8000.102993	13.319898	-0.061534	4.815386
303.571791	8000.165446	13.324903	-0.061539	4.815404
303.483635	8000.255913	13.329907	-0.061523	4.815431
303.611535	8000.159687	13.334912	-0.061546	4.815403
303.680717	8000.207869	13.339917	-0.061559	4.815416
303.679366	8000.153325	13.344922	-0.061559	4.815400
303.656388	8000.222425	13.349927	-0.061555	4.815421
303.542698	8000.220534	13.354931	-0.061534	4.815421
303.785845	8000.101635	13.359936	-0.061579	4.815385
303.757254	8000.195229	13.364941	-0.061573	4.815412
303.715489	8000.227672	13.369946	-0.061566	4.815422
303.659996	8000.192540	13.374951	-0.061555	4.815412
303.730679	8000.238609	13.379955	-0.061568	4.815425
303.702013	8000.091678	13.384960	-0.061563	4.815382
303.634511	8000.246627	13.389965	-0.061550	4.815428
303.710418	8000.289577	13.394970	-0.061565	4.815440
303.744759	8000.209969	13.399975	-0.061571	4.815417
303.419941	8000.244125	13.404979	-0.061510	4.815428
303.592174	8000.109082	13.409984	-0.061542	4.815388
303.557385	8000.161952	13.414989	-0.061536	4.815404
303.628872	8000.120376	13.419994	-0.061549	4.815391
303.504789	8000.033863	13.424999	-0.061526	4.815366
303.665391	8000.145564	13.430003	-0.061556	4.815398
303.744640	7999.959804	13.435008	-0.061571	4.815344
303.578803	8000.283090	13.440013	-0.061540	4.815439
303.738719	7999.954356	13.445018	-0.061569	4.815342
303.667300	8000.113515	13.450023	-0.061556	4.815389
303.558546	8000.220744	13.455027	-0.061536	4.815421
303.618001	7999.986551	13.460032	-0.061547	4.815352
303.902757	8000.292734	13.465037	-0.061600	4.815440
303.861355	7999.929654	13.470042	-0.061592	4.815334
303.721554	8000.142197	13.475047	-0.061566	4.815397
303.711442	8000.038334	13.480051	-0.061564	4.815367
303.653240	8000.163506	13.485056	-0.061553	4.815404
303.534404	8000.157254	13.490061	-0.061531	4.815402
303.447375	7999.918492	13.495066	-0.061515	4.815333
303.633597	8000.038100	13.500071	-0.061550	4.815367
303.636052	8000.093725	13.505075	-0.061550	4.815383
303.609530	8000.067627	13.510080	-0.061545	4.815376
303.560160	8000.206842	13.515085	-0.061536	4.815417
303.610870	8000.143542	13.520090	-0.061545	4.815398
303.556294	8000.190737	13.525095	-0.061535	4.815412
303.451773	8000.323692	13.530099	-0.061516	4.815451
303.700778	8000.148234	13.535104	-0.061562	4.815399
303.639634	8000.238080	13.540109	-0.061551	4.815425
303.678252	8000.186338	13.545114	-0.061558	4.815410
303.711137	8000.215745	13.550119	-0.061564	4.815419
303.587342	8000.114270	13.555123	-0.061541	4.815390
303.602140	8000.131616	13.560128	-0.061543	4.815395
303.629583	8000.151311	13.565133	-0.061548	4.815400
303.552022	8000.133986	13.570138	-0.061534	4.815395
303.591422	8000.195570	13.575143	-0.061541	4.815413
303.860433	7999.992650	13.580147	-0.061591	4.815353
303.595512	8000.084457	13.585152	-0.061542	4.815381
303.675080	8000.152054	13.590157	-0.061557	4.815400
303.775795	7999.948477	13.595162	-0.061575	4.815340
303.781364	8000.132433	13.600167	-0.061576	4.815394
303.666776	7999.960559	13.605171	-0.061555	4.815344
303.766050	7999.966480	13.610176	-0.061573	4.815345
303.653595	8000.113200	13.615181	-0.061553	4.815389
303.681375	8000.014242	13.620186	-0.061558	4.815360
303.541997	8000.076065	13.625191	-0.061532	4.815379
303.574665	8000.062708	13.630195	-0.061538	4.815375
303.599387	8000.096254	13.635200	-0.061542	4.815384
303.486659	8000.193795	13.640205	-0.061521	4.815413
303.592453	8000.096133	13.645210	-0.061541	4.815384
303.516830	8000.093806	13.650215	-0.061527	4.815384
303.404731	8000.318568	13.655219	-0.061506	4.815450
303.532586	8000.220203	13.660224	-0.061530	4.815421
303.615709	8000.312446	13.665229	-0.061545	4.815447
303.720604	8000.082213	13.670234	-0.061565	4.815380
303.638313	8000.128949	13.675239	-0.061549	4.815394
303.579700	8000.222044	13.680243	-0.061539	4.815421
303.609317	8000.189394	13.685248	-0.061544	4.815411
303.686276	8000.223809	13.690253	-0.061558	4.815421
303.459295	8000.014791	13.695258	-0.061516	4.815361
303.635787	8000.159894	13.700263	-0.061549	4.815403
303.734868	8000.109156	13.705267	-0.061567	4.815387
303.797452	8000.043915	13.710272	-0.061579	4.815368
303.766761	8000.175958	13.715277	-0.061573	4.815407
303.666008	8000.025693	13.720282	-0.061554	4.815363
303.641409	8000.071248	13.725287	-0.061550	4.815377
303.611852	8000.343348	13.730291	-0.061544	4.815456
303.614962	8000.077217	13.735296	-0.061545	4.815379
303.464420	8000.214753	13.740301	-0.061517	4.815419
303.417015	8000.189376	13.745306	-0.061508	4.815412
303.537962	8000.298281	13.750311	-0.061530	4.815444
303.401986	8000.219053	13.755315	-0.061505	4.815421
303.487025	8000.317741	13.760320	-0.061521	4.815449
303.538868	8000.222389	13.765325	-0.061530	4.815421
303.623102	8000.049540	13.770330	-0.061546	4.815370
303.429392	8000.215221	13.775335	-0.061510	4.815420
303.432360	8000.266579	13.780339	-0.061511	4.815435
303.876890	8000.081540	13.785344	-0.061593	4.815379
303.713886	8000.097003	13.790349	-0.061563	4.815384
303.669209	8000.160398	13.795354	-0.061554	4.815403
303.817569	7999.997166	13.800359	-0.061582	4.815354
303.727449	8000.080117	13.805363	-0.061565	4.815379
303.705312	7999.841363	13.810368	-0.061561	4.815309
303.680111	8000.126361	13.815373	-0.061556	4.815393
303.728482	7999.945434	13.820378	-0.061565	4.815340
303.673577	8000.139075	13.825383	-0.061555	4.815396
303.596114	8000.191236	13.830387	-0.061541	4.815412
303.868452	8000.123064	13.835392	-0.061591	4.815391
303.681890	8000.215104	13.840397	-0.061557	4.815419
303.686949	8000.087975	13.845402	-0.061557	4.815381
303.852558	8000.101412	13.850407	-0.061588	4.815385
303.815108	8000.136064	13.855411	-0.061581	4.815395
303.786737	8000.129176	13.860416	-0.061576	4.815393
303.548245	8000.162628	13.865421	-0.061532	4.815404
303.591710	8000.096001	13.870426	-0.061540	4.815384
303.582361	8000.185638	13.875431	-0.061538	4.815410
303.639081	8000.036919	13.880435	-0.061548	4.815367
303.548762	8000.079245	13.885440	-0.061531	4.815380
303.728660	8000.082229	13.890445	-0.061565	4.815380
303.530597	8000.121697	13.895450	-0.061528	4.815392
303.692587	7999.993968	13.900455	-0.061558	4.815354
303.839005	8000.190953	13.905459	-0.061585	4.815411
303.799403	8000.084462	13.910464	-0.061578	4.815380
303.648648	8000.170683	13.915469	-0.061550	4.815406
303.891384	8000.259163	13.920474	-0.061595	4.815430
303.817865	8000.194868	13.925479	-0.061581	4.815412
303.684227	8000.225784	13.930483	-0.061556	4.815422
303.941371	8000.082531	13.935488	-0.061604	4.815379
303.768630	7999.968485	13.940493	-0.061572	4.815346
303.689093	8000.126440	13.945498	-0.061557	4.815393
303.697786	7999.881785	13.950503	-0.061559	4.815321
303.647107	8000.320296	13.955507	-0.061549	4.815449
303.871685	8000.027910	13.960512	-0.061591	4.815363
303.933951	8000.240603	13.965517	-0.061603	4.815425
303.861940	7999.962535	13.970522	-0.061589	4.815344
303.844972	8000.133289	13.975527	-0.061586	4.815394
303.720616	7999.967666	13.980531	-0.061563	4.815346
303.868482	7999.960497	13.985536	-0.061590	4.815343
303.788372	8000.027580	13.990541	-0.061575	4.815363
303.613834	8000.030024	13.995546	-0.061543	4.815365
303.635005	8000.105202	14.000551	-0.061547	4.815387
303.906996	8000.256169	14.005555	-0.061598	4.815429
303.840923	8000.115030	14.010560	-0.061585	4.815389
303.627704	8000.270767	14.015565	-0.061545	4.815435
303.778152	8000.042360	14.020570	-0.061573	4.815368
304.079116	8000.021699	14.025575	-0.061629	4.815360
303.722323	7999.984771	14.030579	-0.061563	4.815351
303.880137	8000.002355	14.035584	-0.061592	4.815355
303.811183	7999.995862	14.040589	-0.061579	4.815354
303.812594	8000.020470	14.045594	-0.061580	4.815361
303.858877	8000.001994	14.050599	-0.061588	4.815355
303.997671	8000.086608	14.055603	-0.061614	4.815380
303.747742	7999.914624	14.060608	-0.061567	4.815331
303.730434	8000.167685	14.065613	-0.061564	4.815404
303.914134	7999.960141	14.070618	-0.061598	4.815343
303.731228	7999.935722	14.075623	-0.061564	4.815337
303.675324	8000.063069	14.080627	-0.061554	4.815374
303.959997	7999.928825	14.085632	-0.061607	4.815334
304.038457	8000.110785	14.090637	-0.061621	4.815386
304.007616	7999.971301	14.095642	-0.061616	4.815346
303.910186	8000.076579	14.100647	-0.061597	4.815377
303.837127	7999.940671	14.105651	-0.061584	4.815338
304.070889	7999.913549	14.110656	-0.061627	4.815329
303.992276	8000.054417	14.115661	-0.061613	4.815370
303.874364	8000.046042	14.120666	-0.061591	4.815368
304.069875	7999.966974	14.125671	-0.061627	4.815344
303.973411	8000.043405	14.130675	-0.061609	4.815367
303.837929	7999.927840	14.135680	-0.061584	4.815334
303.818566	8000.034415	14.140685	-0.061580	4.815365
303.823517	7999.938286	14.145690	-0.061581	4.815337
304.003755	7999.896378	14.150695	-0.061614	4.815324
303.961788	7999.904230	14.155699	-0.061607	4.815326
303.867667	8000.029875	14.160704	-0.061589	4.815364
303.931003	8000.064062	14.165709	-0.061601	4.815373
303.779799	8000.046583	14.170714	-0.061573	4.815369
303.990949	7999.997706	14.175719	-0.061612	4.815354
303.738633	8000.066205	14.180723	-0.061565	4.815375
303.747282	8000.081312	14.185728	-0.061567	4.815379
303.858270	8000.131257	14.190733	-0.061587	4.815393
304.086340	8000.001417	14.195738	-0.061630	4.815354
303.832017	7999.939466	14.200743	-0.061582	4.815337
303.776387	8000.041163	14.205747	-0.061572	4.815367
303.889767	7999.939351	14.210752	-0.061593	4.815337
304.051083	8000.041443	14.215757	-0.061623	4.815366
303.952939	8000.036603	14.220762	-0.061605	4.815365
303.959125	7999.976840	14.225767	-0.061606	4.815348
303.975715	8000.095771	14.230771	-0.061609	4.815382
303.791675	7999.856466	14.235776	-0.061574	4.815313
304.007870	7999.953055	14.240781	-0.061615	4.815340
303.986670	8000.068151	14.245786	-0.061611	4.815374
303.790126	7999.890640	14.250791	-0.061574	4.815323
303.848788	7999.935439	14.255795	-0.061585	4.815336
304.021590	7999.570578	14.260800	-0.061617	4.815229
303.968031	7996.303259	14.265805	-0.061605	4.814275
303.927293	7990.668032	14.270810	-0.061593	4.812628
303.969287	7983.962770	14.275815	-0.061597	4.810668
303.736983	7976.636688	14.280819	-0.061549	4.808527
303.686854	7969.036232	14.285824	-0.061535	4.806304
303.881969	7961.210670	14.290829	-0.061566	4.804013
303.934443	7953.315152	14.295834	-0.061570	4.801701
303.827687	7945.418861	14.300839	-0.061545	4.799388
303.501710	7937.437924	14.305843	-0.061479	4.797050
303.718701	7929.440359	14.310848	-0.061514	4.794704
303.657924	7921.341485	14.315853	-0.061498	4.792328
303.627373	7913.326848	14.320858	-0.061487	4.789976
303.625362	7905.414355	14.325863	-0.061481	4.787652
303.629890	7897.362396	14.330867	-0.061477	4.785286
303.499668	7889.396429	14.335872	-0.061447	4.782945
303.402405	7881.370138	14.340877	-0.061424	4.780585
303.577198	7873.407757	14.345882	-0.061451	4.778241
303.591148	7865.433297	14.350887	-0.061449	4.775893
303.556007	7857.360387	14.355891	-0.061437	4.773516
303.448632	7849.326596	14.360896	-0.061412	4.771149
303.149087	7841.316621	14.365901	-0.061351	4.768788
303.234912	7833.375889	14.370906	-0.061361	4.766445
303.392836	7825.405029	14.375911	-0.061386	4.764092
303.174964	7817.376398	14.380915	-0.061340	4.761722
303.039638	7809.379259	14.385920	-0.061309	4.759360
303.086765	7801.394638	14.390925	-0.061313	4.757000
303.026574	7793.323012	14.395930	-0.061296	4.754613
302.895523	7785.316903	14.400935	-0.061267	4.752245
302.977546	7777.227610	14.405939	-0.061277	4.749850
303.175181	7769.348097	14.410944	-0.061308	4.747516
303.063841	7761.279446	14.415949	-0.061282	4.745125
302.989533	7753.356383	14.420954	-0.061263	4.742776
303.057473	7745.360897	14.425959	-0.061271	4.740405
302.952236	7737.322395	14.430963	-0.061246	4.738019
302.933544	7729.333012	14.435968	-0.061237	4.735647
302.873330	7721.290501	14.440973	-0.061221	4.733258
302.811594	7713.278322	14.445978	-0.061204	4.730877
302.815279	7705.332756	14.450983	-0.061199	4.728514
302.844703	7697.248730	14.455987	-0.061200	4.726109
302.909933	7689.331670	14.460992	-0.061207	4.723752
302.660414	7681.280550	14.465997	-0.061155	4.721355
302.460520	7673.287478	14.471002	-0.061112	4.718974
302.485282	7665.390473	14.476007	-0.061112	4.716620
302.537934	7657.309283	14.481011	-0.061116	4.714209
302.511402	7649.269224	14.486016	-0.061106	4.711810
302.529272	7641.282764	14.491021	-0.061104	4.709426
302.697457	7633.247179	14.496026	-0.061130	4.707025
302.429865	7625.277105	14.501031	-0.061075	4.704643
302.481752	7617.287426	14.506035	-0.061080	4.702254
302.668586	7609.282940	14.511040	-0.061109	4.699859
302.548794	7601.346031	14.516045	-0.061082	4.697483
302.373899	7593.306516	14.521050	-0.061044	4.695076
302.436714	7585.300885	14.526055	-0.061050	4.692677
302.408719	7577.244616	14.531059	-0.061040	4.690262
302.341805	7569.297374	14.536064	-0.061022	4.687878
302.340796	7561.218357	14.541069	-0.061017	4.685454
302.491334	7553.299295	14.546074	-0.061039	4.683076
302.447893	7545.269871	14.551079	-0.061026	4.680664
302.024007	7537.268519	14.556083	-0.060942	4.678259
302.104972	7529.272004	14.561088	-0.060952	4.675854
302.030702	7521.233159	14.566093	-0.060933	4.673436
302.157263	7513.136234	14.571098	-0.060951	4.670998
302.018808	7505.201857	14.576103	-0.060920	4.668609
301.942266	7497.191091	14.581107	-0.060900	4.666195
302.013176	7489.267949	14.586112	-0.060908	4.663806
301.899367	7481.238426	14.591117	-0.060882	4.661384
302.047803	7473.238957	14.596122	-0.060904	4.658969
302.120102	7465.255712	14.601127	-0.060913	4.656558
301.961097	7457.227226	14.606131	-0.060878	4.654133
301.961082	7449.215906	14.611136	-0.060872	4.651711
302.018416	7441.159409	14.616141	-0.060878	4.649274
301.809036	7433.204339	14.621146	-0.060834	4.646867
301.689480	7425.200115	14.626151	-0.060806	4.644444
301.674750	7417.231296	14.631155	-0.060798	4.642030
301.823114	7409.207281	14.636160	-0.060821	4.639598
301.633534	7401.291699	14.641165	-0.060780	4.637198
301.616556	7393.201627	14.646170	-0.060772	4.634743
301.912127	7385.178084	14.651175	-0.060821	4.632307
301.726144	7377.117844	14.656179	-0.060781	4.629859
301.740088	7369.197791	14.661184	-0.060779	4.627453
301.607405	7361.156453	14.666189	-0.060749	4.625008
301.540077	7353.207727	14.671194	-0.060731	4.622590
301.516050	7345.178111	14.676199	-0.060721	4.620146
301.495735	7337.173263	14.681203	-0.060712	4.617708
301.502249	7329.160375	14.686208	-0.060708	4.615267
301.452724	7321.170153	14.691213	-0.060694	4.612831
301.485955	7313.106406	14.696218	-0.060695	4.610372
301.617745	7305.199328	14.701223	-0.060714	4.607959
301.408395	7297.123733	14.706227	-0.060670	4.605493
301.424902	7289.197494	14.711232	-0.060668	4.603071
301.394580	7281.177436	14.716237	-0.060657	4.600620
301.114062	7273.157840	14.721242	-0.060599	4.598167
301.148244	7265.189187	14.726247	-0.060600	4.595729
301.061093	7257.095451	14.731251	-0.060579	4.593251
301.024377	7249.105902	14.736256	-0.060567	4.590804
300.955190	7241.104399	14.741261	-0.060549	4.588352
300.970931	7233.082615	14.746266	-0.060546	4.585892
301.030894	7225.165754	14.751271	-0.060552	4.583463
301.131666	7217.146218	14.756275	-0.060566	4.581001
300.920869	7209.184599	14.761280	-0.060521	4.578556
301.223455	7201.140602	14.766285	-0.060573	4.576084
301.052905	7193.124562	14.771290	-0.060536	4.573619
300.761812	7185.095033	14.776295	-0.060476	4.571149
300.737470	7177.095445	14.781299	-0.060466	4.568686
300.790362	7169.102956	14.786304	-0.060471	4.566225
300.908672	7161.132755	14.791309	-0.060488	4.563769
300.848407	7153.104736	14.796314	-0.060471	4.561294
300.871496	7145.124274	14.801319	-0.060470	4.558832
300.880844	7137.124921	14.806323	-0.060467	4.556363
300.585803	7129.160583	14.811328	-0.060407	4.553904
300.660573	7121.099947	14.816333	-0.060415	4.551413
300.599304	7113.059509	14.821338	-0.060399	4.548927
300.715430	7105.077088	14.826343	-0.060415	4.546459
300.480029	7097.108884	14.831347	-0.060366	4.543992
300.579146	7089.143282	14.836352	-0.060379	4.541526
300.524224	7081.093187	14.841357	-0.060364	4.539032
300.446371	7073.105071	14.846362	-0.060344	4.536555
300.660006	7065.115572	14.851367	-0.060378	4.534078
300.522845	7057.066170	14.856371	-0.060348	4.531579
300.463536	7049.094148	14.861376	-0.060331	4.529104
300.384580	7041.099520	14.866381	-0.060311	4.526620
300.346383	7033.083941	14.871386	-0.060299	4.524128
300.376614	7025.143572	14.876391	-0.060299	4.521659
300.200264	7017.085657	14.881395	-0.060261	4.519151
300.347514	7009.148188	14.886400	-0.060284	4.516680
300.158427	7001.091327	14.891405	-0.060243	4.514170
300.071822	6992.984164	14.896410	-0.060222	4.511642
300.048520	6985.024188	14.901415	-0.060212	4.509160
300.069339	6977.041248	14.906419	-0.060211	4.506669
300.092012	6969.059707	14.911424	-0.060210	4.504177
300.166022	6961.134096	14.916429	-0.060218	4.501701
299.999847	6953.028199	14.921434	-0.060182	4.499167
299.851638	6945.111407	14.926439	-0.060149	4.496690
299.857428	6937.051015	14.931443	-0.060145	4.494168
300.004467	6929.038696	14.936448	-0.060167	4.491660
299.723626	6921.066757	14.941453	-0.060110	4.489162
299.685891	6913.031295	14.946458	-0.060097	4.486643
299.833892	6905.036345	14.951463	-0.060120	4.484136
299.757032	6897.049082	14.956467	-0.060100	4.481629
299.684515	6889.048388	14.961472	-0.060081	4.479117
299.615838	6881.080992	14.966477	-0.060063	4.476614
299.415701	6873.030127	14.971482	-0.060021	4.474082
299.614550	6865.051016	14.976487	-0.060053	4.471574
299.782926	6857.013175	14.981491	-0.060079	4.469045
299.704266	6849.046049	14.986496	-0.060059	4.466536
299.551801	6841.027814	14.991501	-0.060025	4.464009
299.458325	6833.042213	14.996506	-0.060003	4.461492
299.662843	6825.052688	15.001511	-0.060035	4.458973
299.435343	6817.050059	15.006515	-0.059988	4.456446
299.629096	6809.059763	15.011520	-0.060019	4.453924
299.597858	6800.994726	15.016525	-0.060008	4.451376
299.503463	6792.964745	15.021530	-0.059985	4.448837
299.416377	6785.002451	15.026535	-0.059963	4.446318
299.230459	6777.013453	15.031539	-0.059923	4.443789
299.312577	6769.016676	15.036544	-0.059933	4.441257
299.263206	6761.012406	15.041549	-0.059919	4.438721
299.111692	6753.022002	15.046554	-0.059886	4.436187
299.232462	6745.000009	15.051559	-0.059903	4.433643
299.054828	6736.972001	15.056563	-0.059864	4.431094
299.094891	6728.962313	15.061568	-0.059867	4.428551
298.947457	6720.936340	15.066573	-0.059834	4.426000
299.040292	6712.961627	15.071578	-0.059846	4.423465
299.125326	6704.955272	15.076583	-0.059857	4.420918
299.125806	6696.982223	15.081587	-0.059851	4.418380
299.057817	6688.967761	15.086592	-0.059834	4.415827
299.025087	6680.954490	15.091597	-0.059822	4.413273
299.061376	6672.930125	15.096602	-0.059824	4.410715
298.896084	6664.984013	15.101607	-0.059788	4.408179
298.842286	6656.964513	15.106611	-0.059772	4.405619
298.772032	6649.035956	15.111616	-0.059754	4.403086
298.734214	6640.994282	15.116621	-0.059742	4.400515
298.672544	6633.030922	15.121626	-0.059725	4.397968
298.792276	6624.991147	15.126631	-0.059742	4.395396
298.559069	6616.950298	15.131635	-0.059694	4.392821
298.741855	6608.934443	15.136640	-0.059722	4.390254
298.516669	6600.989652	15.141645	-0.059675	4.387706
298.359626	6592.939393	15.146650	-0.059641	4.385123
298.574223	6585.011873	15.151655	-0.059675	4.382580
298.554752	6576.945313	15.156659	-0.059666	4.379990
298.575303	6569.031444	15.161664	-0.059665	4.377447
298.396718	6560.990857	15.166669	-0.059627	4.374861
298.497042	6552.994596	15.171674	-0.059640	4.372290
298.326831	6544.956652	15.176679	-0.059603	4.369702
298.195857	6536.980954	15.181683	-0.059573	4.367132
298.308545	6528.962763	15.186688	-0.059589	4.364549
298.307846	6521.034704	15.191693	-0.059584	4.361993
298.243681	6512.990641	15.196698	-0.059567	4.359397
298.126647	6505.006579	15.201703	-0.059540	4.356819
298.360107	6496.921807	15.206707	-0.059578	4.354209
298.307366	6488.847516	15.211712	-0.059563	4.351599
298.258593	6480.896723	15.216717	-0.059548	4.349028
298.196240	6472.919108	15.221722	-0.059532	4.346446
298.388045	6464.961283	15.226727	-0.059562	4.343870
297.898462	6456.949999	15.231731	-0.059466	4.341272
297.943082	6448.947929	15.236736	-0.059469	4.338678
297.976848	6440.971070	15.241741	-0.059470	4.336091
298.085749	6432.919472	15.246746	-0.059485	4.333478
297.926281	6424.940940	15.251751	-0.059450	4.330886
297.834489	6416.953300	15.256755	-0.059428	4.328290
297.829972	6408.948428	15.261760	-0.059421	4.325687
297.756255	6400.953750	15.266765	-0.059402	4.323085
297.643921	6392.936981	15.271770	-0.059376	4.320475
297.800356	6384.994757	15.276775	-0.059400	4.317889
297.636705	6376.939057	15.281779	-0.059364	4.315262
297.749196	6368.954749	15.286784	-0.059380	4.312659
297.706360	6360.886993	15.291789	-0.059367	4.310026
297.494121	6352.933276	15.296794	-0.059322	4.307427
297.578741	6344.940231	15.301799	-0.059333	4.304816
297.560992	6336.913381	15.306803	-0.059324	4.302192
297.508465	6328.919942	15.311808	-0.059309	4.299576
297.490971	6320.992530	15.316813	-0.059301	4.296981
297.585022	6312.894741	15.321818	-0.059313	4.294330
297.719592	6304.912356	15.326823	-0.059333	4.291715
297.568174	6296.894245	15.331827	-0.059299	4.289084
297.313355	6288.927442	15.336832	-0.059247	4.286468
297.242213	6280.945809	15.341837	-0.059228	4.283847
297.301132	6272.915471	15.346842	-0.059234	4.281209
297.411956	6264.973244	15.351847	-0.059249	4.278599
297.321475	6256.940404	15.356851	-0.059227	4.275956
297.123711	6248.907756	15.361856	-0.059185	4.273310
297.069589	6240.853696	15.366861	-0.059170	4.270657
297.086002	6232.864381	15.371866	-0.059167	4.268024
297.277930	6224.871583	15.376871	-0.059198	4.265390
297.028669	6216.888752	15.381875	-0.059146	4.262754
297.119572	6208.904702	15.386880	-0.059158	4.260119
297.111952	6200.925384	15.391885	-0.059151	4.257483
297.081814	6192.905368	15.396890	-0.059141	4.254831
296.929653	6184.889935	15.401895	-0.059107	4.252178
296.904514	6176.856274	15.406899	-0.059097	4.249519
296.935447	6168.925051	15.411904	-0.059098	4.246892
296.681617	6160.907796	15.416909	-0.059045	4.244233
296.753593	6152.926986	15.421914	-0.059053	4.241587
296.966608	6144.934916	15.426919	-0.059088	4.238937
296.689723	6136.947628	15.431923	-0.059031	4.236283
296.732768	6128.954407	15.436928	-0.059034	4.233627
296.726884	6120.898134	15.441933	-0.059027	4.230949
296.658896	6112.913514	15.446938	-0.059009	4.228292
296.615352	6104.891041	15.451943	-0.058996	4.225621
296.387725	6096.939996	15.456947	-0.058948	4.222971
296.536383	6088.877066	15.461952	-0.058971	4.220285
296.495150	6080.965259	15.466957	-0.058958	4.217646
296.443803	6072.904418	15.471962	-0.058943	4.214955
296.329768	6064.939440	15.476967	-0.058917	4.212294
296.159680	6056.888785	15.481971	-0.058880	4.209603
296.271869	6048.923386	15.486976	-0.058895	4.206940
296.318819	6040.929554	15.491981	-0.058899	4.204266
296.270228	6032.941896	15.496986	-0.058885	4.201592
296.330285	6024.975525	15.501991	-0.058891	4.198924
296.146296	6016.929690	15.506995	-0.058851	4.196225
296.382470	6008.855367	15.512000	-0.058890	4.193519
296.366350	6000.804417	15.517005	-0.058881	4.190817
296.142992	5992.838715	15.522010	-0.058835	4.188139
296.127491	5984.910521	15.527015	-0.058826	4.185474
296.022522	5976.900263	15.532019	-0.058802	4.182779
296.024891	5968.896359	15.537024	-0.058797	4.180086
296.063850	5960.917741	15.542029	-0.058799	4.177400
295.978136	5952.892778	15.547034	-0.058778	4.174695
296.025632	5944.922333	15.552039	-0.058781	4.172008
295.948270	5936.831664	15.557043	-0.058762	4.169278
296.039571	5928.928344	15.562048	-0.058773	4.166610
295.987535	5920.944350	15.567053	-0.058758	4.163913
295.816219	5912.915132	15.572058	-0.058721	4.161197
295.853589	5904.941321	15.577063	-0.058723	4.158500
295.791752	5896.906001	15.582067	-0.058706	4.155779
295.801544	5888.884562	15.587072	-0.058703	4.153063
295.845809	5880.857051	15.592077	-0.058706	4.150342
295.731549	5872.851366	15.597082	-0.058679	4.147626
295.688383	5864.863200	15.602087	-0.058666	4.144914
295.461694	5856.906060	15.607091	-0.058619	4.142210
295.558903	5848.886705	15.612096	-0.058631	4.139486
295.651737	5840.904876	15.617101	-0.058644	4.136773
295.459428	5832.877942	15.622106	-0.058602	4.134039
295.325722	5824.874456	15.627111	-0.058572	4.131312
295.345666	5816.871663	15.632115	-0.058571	4.128586
295.184138	5808.867954	15.637120	-0.058535	4.125855
295.355657	5800.897667	15.642125	-0.058562	4.123138
295.353569	5792.902398	15.647130	-0.058557	4.120408
295.306780	5784.968904	15.652135	-0.058543	4.117697
295.341505	5776.889727	15.657139	-0.058544	4.114936
295.226109	5768.857164	15.662144	-0.058517	4.112187
295.208206	5760.821804	15.667149	-0.058508	4.109436
295.125500	5752.865356	15.672154	-0.058488	4.106710
295.189470	5744.904109	15.677159	-0.058495	4.103982
295.261349	5736.868672	15.682163	-0.058503	4.101226
295.035504	5728.887319	15.687168	-0.058455	4.098484
294.975532	5720.940450	15.692173	-0.058439	4.095754
295.112524	5712.879584	15.697178	-0.058459	4.092985
294.992143	5704.871354	15.702183	-0.058432	4.090229
294.832909	5696.900934	15.707187	-0.058397	4.087484
294.959282	5688.917454	15.712192	-0.058415	4.084737
294.935296	5680.973321	15.717197	-0.058405	4.081999
294.844466	5672.943068	15.722202	-0.058383	4.079228
294.836139	5665.000941	15.727207	-0.058376	4.076487
294.947921	5656.874974	15.732211	-0.058392	4.073683
294.837074	5648.889982	15.737216	-0.058366	4.070922
294.751467	5640.916658	15.742221	-0.058345	4.068164
294.693329	5632.887237	15.747226	-0.058329	4.065385
294.676044	5624.967122	15.752231	-0.058320	4.062642
294.557661	5616.942134	15.757235	-0.058293	4.059860
294.661360	5608.939638	15.762240	-0.058307	4.057086
294.734799	5600.915051	15.767245	-0.058315	4.054303
294.653567	5592.919474	15.772250	-0.058295	4.051526
294.505096	5584.950199	15.777255	-0.058262	4.048755
294.397679	5576.928174	15.782259	-0.058237	4.045964
294.321643	5568.974993	15.787264	-0.058218	4.043196
294.428812	5560.969326	15.792269	-0.058232	4.040410
294.234713	5552.952427	15.797274	-0.058191	4.037614
294.446325	5544.934536	15.802279	-0.058225	4.034821
294.093458	5536.844425	15.807283	-0.058154	4.031993
294.223535	5528.858160	15.812288	-0.058173	4.029207
294.285812	5520.886569	15.817293	-0.058179	4.026423
294.157565	5512.872544	15.822298	-0.058150	4.023619
294.155326	5504.935361	15.827303	-0.058145	4.020842
294.300691	5496.915167	15.832307	-0.058166	4.018036
294.198308	5488.891871	15.837312	-0.058142	4.015224
294.055441	5480.938355	15.842317	-0.058110	4.012433
293.988176	5472.866983	15.847322	-0.058093	4.009600
294.095003	5464.958893	15.852327	-0.058107	4.006825
293.787716	5456.907864	15.857331	-0.058045	4.003992
293.797428	5448.931797	15.862336	-0.058041	4.001187
293.927279	5440.957650	15.867341	-0.058060	3.998384
293.653042	5432.940085	15.872346	-0.058004	3.995557
293.962900	5424.929064	15.877351	-0.058056	3.992739
293.977104	5416.867227	15.882355	-0.058054	3.989897
293.882919	5408.919622	15.887360	-0.058031	3.987091
293.792886	5400.923549	15.892365	-0.058009	3.984266
293.740608	5392.956167	15.897370	-0.057994	3.981450
293.788070	5384.920949	15.902375	-0.057998	3.978610
293.726997	5376.944173	15.907379	-0.057981	3.975786
293.835433	5368.943081	15.912384	-0.057996	3.972955
293.851751	5360.906210	15.917389	-0.057994	3.970107
293.718591	5352.926208	15.922394	-0.057964	3.967275
293.420556	5344.971259	15.927399	-0.057903	3.964447
293.476885	5336.955065	15.932403	-0.057908	3.961602
293.591863	5328.978681	15.937408	-0.057924	3.958769
293.513021	5321.011172	15.942413	-0.057905	3.955934
293.396220	5312.938128	15.947418	-0.057877	3.953059
293.656518	5304.917520	15.952423	-0.057921	3.950207
293.300121	5296.937967	15.957427	-0.057849	3.947357
293.222490	5288.931419	15.962432	-0.057829	3.944500
293.338171	5280.993774	15.967437	-0.057846	3.941669
293.162313	5272.974835	15.972442	-0.057808	3.938802
293.113569	5265.023617	15.977447	-0.057793	3.935959
292.878410	5256.971412	15.982451	-0.057744	3.933075
292.985003	5248.980500	15.987456	-0.057759	3.930216
292.999484	5241.004342	15.992461	-0.057756	3.927359
292.925989	5232.946139	15.997466	-0.057737	3.924469
293.238857	5225.025743	16.002471	-0.057791	3.921633
292.899963	5217.000598	16.007475	-0.057722	3.918746
292.685682	5209.023814	16.012480	-0.057677	3.915876
293.034131	5201.019852	16.017485	-0.057737	3.913005
293.084296	5192.923311	16.022490	-0.057741	3.910093
293.000502	5185.000906	16.027495	-0.057720	3.907239
292.673774	5176.987769	16.032499	-0.057654	3.904345
292.761241	5169.019794	16.037504	-0.057665	3.901474
292.710185	5161.032876	16.042509	-0.057650	3.898591
292.675222	5152.991425	16.047514	-0.057638	3.895686
292.762021	5144.997095	16.052519	-0.057649	3.892798
292.607042	5136.963594	16.057523	-0.057615	3.889890
292.486698	5128.997287	16.062528	-0.057588	3.887004
292.361857	5120.998420	16.067533	-0.057559	3.884104
292.488047	5113.022345	16.072538	-0.057577	3.881216
292.257389	5105.046294	16.077543	-0.057529	3.878318
292.517713	5097.003540	16.082547	-0.057572	3.875403
292.350412	5088.807654	16.087552	-0.057536	3.872422
292.360401	5080.805135	16.092557	-0.057532	3.869513
292.150118	5072.898639	16.097562	-0.057488	3.866632
292.361237	5064.939192	16.102567	-0.057522	3.863738
292.109294	5056.951833	16.107571	-0.057470	3.860822
292.179197	5048.979504	16.112576	-0.057478	3.857916
292.193698	5040.997395	16.117581	-0.057475	3.855003
292.135965	5032.994546	16.122586	-0.057459	3.852079
292.227378	5025.014303	16.127591	-0.057471	3.849164
292.091566	5016.983600	16.132595	-0.057441	3.846224
292.019247	5008.986251	16.137600	-0.057422	3.843295
291.812652	5001.044296	16.142605	-0.057378	3.840381
291.571110	4993.056800	16.147610	-0.057328	3.837448
291.854793	4985.031453	16.152615	-0.057376	3.834509
291.759897	4977.017411	16.157619	-0.057353	3.831564
291.814320	4969.036770	16.162624	-0.057358	3.828633
291.875041	4961.030468	16.167629	-0.057364	3.825690
291.961229	4953.023764	16.172634	-0.057374	3.822745
292.033861	4945.087525	16.177639	-0.057383	3.819823
291.894671	4937.078929	16.182643	-0.057352	3.816868
291.926579	4929.086182	16.187648	-0.057352	3.813920
291.859372	4921.058010	16.192653	-0.057334	3.810955
291.627876	4913.081991	16.197658	-0.057286	3.808003
291.743558	4905.076827	16.202663	-0.057302	3.805046
291.704597	4897.122311	16.207667	-0.057290	3.802101
291.419800	4889.120152	16.212672	-0.057232	3.799132
291.484130	4881.130764	16.217677	-0.057238	3.796172
291.453692	4873.076620	16.222682	-0.057227	3.793184
291.512503	4865.054658	16.227687	-0.057233	3.790207
291.328295	4857.093754	16.232691	-0.057194	3.787246
291.546298	4849.038781	16.237696	-0.057229	3.784256
291.474799	4841.136580	16.242701	-0.057210	3.781314
291.324600	4833.091923	16.247706	-0.057177	3.778315
291.344432	4825.121362	16.252711	-0.057176	3.775345
291.253011	4817.102711	16.257715	-0.057153	3.772352
291.217451	4809.089592	16.262720	-0.057142	3.769361
291.216862	4801.145057	16.267725	-0.057136	3.766393
291.309186	4793.069230	16.272730	-0.057148	3.763376
291.334751	4785.122371	16.277735	-0.057148	3.760403
291.071588	4777.114513	16.282739	-0.057093	3.757398
291.231139	4769.082978	16.287744	-0.057118	3.754392
291.226351	4761.117894	16.292749	-0.057112	3.751405
290.931119	4753.095687	16.297754	-0.057052	3.748387
291.025105	4745.121504	16.302759	-0.057064	3.745393
290.975988	4737.111952	16.307763	-0.057049	3.742381
290.837126	4729.129422	16.312768	-0.057018	3.739374
290.831446	4721.202204	16.317773	-0.057012	3.736389
290.859093	4713.116930	16.322778	-0.057012	3.733342
290.853256	4705.122276	16.327783	-0.057006	3.730327
290.701504	4697.147472	16.332787	-0.056972	3.727313
290.887714	4689.104026	16.337792	-0.057001	3.724279
291.114356	4681.170958	16.342797	-0.057038	3.721285
290.780613	4673.185982	16.347802	-0.056971	3.718255
290.612484	4665.211882	16.352807	-0.056935	3.715231
290.899987	4657.105547	16.357811	-0.056983	3.712165
290.594229	4649.096706	16.362816	-0.056921	3.709120
290.631318	4641.120901	16.367821	-0.056922	3.706093
290.704455	4633.145157	16.372826	-0.056931	3.703064
290.796263	4625.194392	16.377831	-0.056943	3.700043
290.395896	4617.224815	16.382835	-0.056863	3.697000
290.372313	4609.195530	16.387840	-0.056853	3.693941
290.720376	4601.167338	16.392845	-0.056913	3.690889
290.535738	4593.201987	16.397850	-0.056873	3.687846
290.612491	4585.218679	16.402855	-0.056882	3.684799
290.325432	4577.248896	16.407859	-0.056823	3.681746
290.443553	4569.272810	16.412864	-0.056840	3.678699
290.368814	4561.248473	16.417869	-0.056821	3.675625
290.406696	4553.188336	16.422874	-0.056823	3.672538
290.451611	4545.214253	16.427879	-0.056826	3.669481
290.001353	4537.247552	16.432883	-0.056737	3.666413
290.013813	4529.250040	16.437888	-0.056734	3.663341
290.153182	4521.266081	16.442893	-0.056755	3.660276
290.162053	4513.268400	16.447898	-0.056751	3.657199
289.978959	4505.280777	16.452903	-0.056712	3.654118
290.028471	4497.243631	16.457907	-0.056716	3.651022
289.955312	4489.239472	16.462912	-0.056697	3.647933
289.774434	4481.262453	16.467917	-0.056658	3.644849
289.621074	4473.290379	16.472922	-0.056624	3.641765
289.830088	4465.288850	16.477927	-0.056658	3.638676
289.695080	4457.290400	16.482931	-0.056627	3.635577
289.591518	4449.252345	16.487936	-0.056603	3.632460
289.744853	4441.237992	16.492941	-0.056626	3.629357
289.726824	4433.253637	16.497946	-0.056618	3.626259
289.731530	4425.285782	16.502951	-0.056613	3.623165
289.731611	4417.276889	16.507955	-0.056608	3.620052
289.773706	4409.315254	16.512960	-0.056611	3.616956
289.674334	4401.315094	16.517965	-0.056587	3.613838
289.450709	4393.283424	16.522970	-0.056540	3.610702
289.592602	4385.334542	16.527975	-0.056561	3.607606
289.444863	4377.328275	16.532979	-0.056528	3.604476
289.335876	4369.402948	16.537984	-0.056503	3.601377
289.412749	4361.377847	16.542989	-0.056512	3.598240
289.329771	4353.349641	16.547994	-0.056491	3.595096
289.347695	4345.362677	16.552999	-0.056489	3.591968
289.273777	4337.343121	16.558003	-0.056470	3.588821
289.376981	4329.355218	16.563008	-0.056484	3.585690
289.299088	4321.415973	16.568013	-0.056465	3.582569
288.979118	4313.395685	16.573018	-0.056400	3.579407
288.991460	4305.461545	16.578023	-0.056397	3.576286
288.973194	4297.402644	16.583027	-0.056388	3.573112
288.632581	4289.404601	16.588032	-0.056320	3.569950
288.800590	4281.434217	16.593037	-0.056346	3.566810
288.780185	4273.417469	16.598042	-0.056337	3.563644
288.840528	4265.459545	16.603047	-0.056343	3.560501
288.839283	4257.477680	16.608051	-0.056337	3.557343
288.887191	4249.419652	16.613056	-0.056341	3.554155
288.745014	4241.351475	16.618061	-0.056309	3.550953
288.709270	4233.368470	16.623066	-0.056297	3.547786
288.961481	4225.353010	16.628071	-0.056339	3.544612
288.680629	4217.451331	16.633075	-0.056281	3.541464
288.782834	4209.426802	16.638080	-0.056295	3.538276
288.664145	4201.473929	16.643085	-0.056268	3.535106
288.472237	4193.422551	16.648090	-0.056227	3.531893
288.357878	4185.437675	16.653095	-0.056200	3.528705
288.272104	4177.429754	16.658099	-0.056179	3.525507
288.463749	4169.472867	16.663104	-0.056210	3.522334
288.484907	4161.475203	16.668109	-0.056208	3.519136
288.333010	4153.489463	16.673114	-0.056175	3.515936
288.515555	4145.490096	16.678119	-0.056203	3.512737
288.461824	4137.474075	16.683123	-0.056188	3.509521
288.313512	4129.496825	16.688128	-0.056155	3.506315
288.357633	4121.502753	16.693133	-0.056158	3.503106
288.459958	4113.488977	16.698138	-0.056172	3.499887
288.384499	4105.565351	16.703143	-0.056153	3.496696
288.167667	4097.553865	16.708147	-0.056107	3.493462
288.100211	4089.521990	16.713152	-0.056089	3.490222
288.112513	4081.569473	16.718157	-0.056087	3.487013
288.034990	4073.569515	16.723162	-0.056067	3.483779
288.211434	4065.599511	16.728167	-0.056094	3.480563
288.150896	4057.626944	16.733171	-0.056078	3.477334
287.875570	4049.590954	16.738176	-0.056021	3.474071
288.006263	4041.555892	16.743181	-0.056041	3.470817
287.885992	4033.591296	16.748186	-0.056013	3.467581
287.796813	4025.597917	16.753191	-0.055991	3.464332
287.654296	4017.641669	16.758195	-0.055959	3.461092
287.887241	4009.629175	16.763200	-0.055997	3.457839
287.728560	4001.627934	16.768205	-0.055963	3.454575
287.542012	3993.661831	16.773210	-0.055923	3.451321
287.539006	3985.644199	16.778215	-0.055917	3.448048
287.679042	3977.611939	16.783219	-0.055938	3.444772
287.679736	3969.652726	16.788224	-0.055933	3.441517
287.569845	3961.686382	16.793229	-0.055907	3.438253
287.632446	3953.659548	16.798234	-0.055913	3.434967
287.574826	3945.669197	16.803239	-0.055897	3.431689
287.544162	3937.656940	16.808243	-0.055886	3.428399
287.376140	3929.667442	16.813248	-0.055850	3.425111
287.421880	3921.712160	16.818253	-0.055853	3.421841
287.357014	3913.711405	16.823258	-0.055836	3.418545
287.318430	3905.738953	16.828263	-0.055823	3.415259
287.318759	3897.741473	16.833267	-0.055818	3.411961
287.431222	3889.705400	16.838272	-0.055834	3.408647
287.509554	3881.742606	16.843277	-0.055843	3.405359
287.333554	3873.771679	16.848282	-0.055805	3.402056
287.420635	3865.786626	16.853287	-0.055816	3.398753
287.137426	3857.802625	16.858291	-0.055758	3.395435
287.170557	3849.707525	16.863296	-0.055759	3.392077
287.185733	3841.742171	16.868301	-0.055757	3.388770
287.075953	3833.751572	16.873306	-0.055731	3.385445
287.220868	3825.769879	16.878311	-0.055753	3.382129
286.994857	3817.821340	16.883315	-0.055706	3.378811
286.870649	3809.828675	16.888320	-0.055677	3.375474
286.840697	3801.837459	16.893325	-0.055666	3.372138
286.783649	3793.818379	16.898330	-0.055651	3.368787
286.952854	3785.820830	16.903335	-0.055677	3.365449
286.601206	3777.891370	16.908339	-0.055606	3.362117
286.627413	3769.880927	16.913344	-0.055606	3.358762
286.825552	3761.894950	16.918349	-0.055637	3.355420
286.603730	3753.864571	16.923354	-0.055591	3.352041
286.543204	3745.888618	16.928359	-0.055574	3.348687
286.571619	3737.861065	16.933363	-0.055574	3.345311
286.672693	3729.890142	16.938368	-0.055588	3.341958
286.660658	3721.914798	16.943373	-0.055580	3.338596
286.544182	3713.921098	16.948378	-0.055554	3.335219
286.489077	3705.923546	16.953383	-0.055538	3.331839
286.471737	3697.929360	16.958387	-0.055530	3.328459
286.406591	3689.933491	16.963392	-0.055512	3.325072
286.600903	3681.985605	16.968397	-0.055543	3.321712
286.212010	3674.008750	16.973402	-0.055466	3.318315
286.175785	3666.013530	16.978407	-0.055454	3.314919
286.004831	3658.008338	16.983411	-0.055416	3.311511
286.290907	3649.973150	16.988416	-0.055464	3.308104
286.077265	3641.993445	16.993421	-0.055419	3.304698
285.874701	3634.059884	16.998426	-0.055377	3.301308
286.040871	3626.053399	17.003431	-0.055402	3.297898
286.157941	3618.025909	17.008435	-0.055419	3.294473
286.058916	3610.031191	17.013440	-0.055395	3.291051
286.147198	3602.054988	17.018445	-0.055406	3.287640
285.990124	3594.043572	17.023450	-0.055372	3.284201
286.049193	3586.112787	17.028455	-0.055378	3.280802
285.942482	3578.136148	17.033459	-0.055353	3.277373
285.778091	3570.119420	17.038464	-0.055317	3.273920
285.512108	3562.131333	17.043469	-0.055262	3.270473
285.839116	3554.100744	17.048474	-0.055318	3.267026
285.817403	3546.128363	17.053479	-0.055308	3.263588
285.556337	3538.150126	17.058483	-0.055254	3.260133
285.630225	3530.162079	17.063488	-0.055263	3.256685
285.600577	3522.173930	17.068493	-0.055252	3.253228
285.532720	3514.144480	17.073498	-0.055234	3.249748
285.624222	3506.191040	17.078503	-0.055246	3.246304
285.565781	3498.210952	17.083507	-0.055230	3.242839
285.353144	3490.228555	17.088512	-0.055185	3.239362
285.695886	3482.275802	17.093517	-0.055244	3.235917
285.346635	3474.200708	17.098522	-0.055173	3.232388
285.359038	3466.196868	17.103527	-0.055171	3.228900
285.386457	3458.191692	17.108531	-0.055170	3.225408
285.420635	3450.231690	17.113536	-0.055172	3.221933
285.457495	3442.246473	17.118541	-0.055173	3.218443
285.174233	3434.277147	17.123546	-0.055115	3.214943
285.198288	3426.312652	17.128551	-0.055114	3.211453
285.096671	3418.325264	17.133555	-0.055090	3.207945
285.117650	3410.288903	17.138560	-0.055089	3.204417
285.248635	3402.357432	17.143565	-0.055108	3.200935
285.036334	3394.361458	17.148570	-0.055063	3.197407
284.952997	3386.383405	17.153575	-0.055043	3.193888
285.150836	3378.325869	17.158579	-0.055074	3.190342
284.866191	3370.377648	17.163584	-0.055016	3.186820
285.053797	3362.384729	17.168589	-0.055046	3.183294
284.889720	3354.390562	17.173594	-0.055010	3.179749
284.998343	3346.433439	17.178599	-0.055025	3.176228
285.008001	3338.413009	17.183603	-0.055021	3.172671
284.891754	3330.421439	17.188608	-0.054994	3.169117
284.874201	3322.458138	17.193613	-0.054986	3.165576
284.589224	3314.500196	17.198618	-0.054928	3.162022
284.811730	3306.498630	17.203623	-0.054964	3.158467
284.759459	3298.506786	17.208627	-0.054949	3.154900
284.580024	3290.477001	17.213632	-0.054910	3.151306
284.530326	3282.498947	17.218637	-0.054896	3.147737
284.478080	3274.492573	17.223642	-0.054881	3.144151
284.484662	3266.520239	17.228647	-0.054877	3.140579
284.292636	3258.577161	17.233651	-0.054836	3.137007
284.376259	3250.539706	17.238656	-0.054846	3.133400
284.467814	3242.556481	17.243661	-0.054858	3.129815
284.179244	3234.576913	17.248666	-0.054799	3.126210
284.229516	3226.636876	17.253671	-0.054803	3.122634
284.178505	3218.637116	17.258675	-0.054788	3.119022
284.019624	3210.678083	17.263680	-0.054754	3.115419
284.169571	3202.665878	17.268685	-0.054776	3.111802
284.344969	3194.620410	17.273690	-0.054804	3.108168
284.247993	3186.654146	17.278695	-0.054780	3.104552
284.093736	3178.713946	17.283699	-0.054746	3.100941
284.257220	3170.718943	17.288704	-0.054772	3.097316
284.229884	3162.729069	17.293709	-0.054761	3.093680
283.761821	3154.729248	17.298714	-0.054669	3.090015
283.873090	3146.772430	17.303719	-0.054684	3.086392
283.753354	3138.789463	17.308723	-0.054657	3.082742
283.783462	3130.779684	17.313728	-0.054657	3.079083
283.967613	3122.823111	17.318733	-0.054686	3.075450
283.801407	3114.756174	17.323738	-0.054650	3.071747
283.761526	3106.765096	17.328743	-0.054637	3.068079
283.746437	3098.771556	17.333747	-0.054629	3.064407
283.641246	3090.832100	17.338752	-0.054605	3.060752
283.664494	3082.851079	17.343757	-0.054604	3.057079
283.492872	3074.864429	17.348762	-0.054567	3.053389
283.476118	3066.860112	17.353767	-0.054558	3.049695
283.478890	3058.906039	17.358771	-0.054553	3.046020
283.425265	3050.926914	17.363776	-0.054538	3.042326
283.499361	3042.961825	17.368781	-0.054547	3.038641
283.286892	3034.976151	17.373786	-0.054502	3.034928
283.335416	3026.944391	17.378791	-0.054506	3.031201
283.254332	3018.958776	17.383795	-0.054485	3.027485
283.185851	3010.987731	17.388800	-0.054467	3.023771
283.357707	3003.010818	17.393805	-0.054494	3.020062
283.250627	2995.057387	17.398810	-0.054469	3.016346
283.072129	2987.059180	17.403815	-0.054431	3.012601
282.979543	2979.074007	17.408819	-0.054408	3.008862
282.836826	2971.077431	17.413824	-0.054376	3.005110
282.872594	2963.134673	17.418829	-0.054378	3.001387
282.735001	2955.148930	17.423834	-0.054347	2.997631
282.703454	2947.149452	17.428839	-0.054336	2.993869
282.597566	2939.124830	17.433843	-0.054311	2.990086
282.721538	2931.131060	17.438848	-0.054329	2.986325
282.657353	2923.175223	17.443853	-0.054312	2.982568
282.742142	2915.171326	17.448858	-0.054322	2.978791
282.676403	2907.225247	17.453863	-0.054305	2.975028
282.831977	2899.214895	17.458867	-0.054328	2.971242
282.628791	2891.226753	17.463872	-0.054285	2.967443
282.440511	2883.291369	17.468877	-0.054245	2.963665
282.673782	2875.275652	17.473882	-0.054283	2.959866
282.616882	2867.334094	17.478887	-0.054267	2.956082
282.440523	2859.316131	17.483891	-0.054229	2.952251
282.647649	2851.284908	17.488896	-0.054263	2.948428
282.588196	2843.354192	17.493901	-0.054246	2.944634
282.521581	2835.388869	17.498906	-0.054229	2.940819
282.491300	2827.401978	17.503911	-0.054218	2.936990
282.553432	2819.389460	17.508915	-0.054224	2.933149
282.368864	2811.411685	17.513920	-0.054185	2.929306
282.387062	2803.458666	17.518925	-0.054183	2.925481
282.230481	2795.478799	17.523930	-0.054148	2.921629
282.110321	2787.534659	17.528935	-0.054121	2.917791
282.087505	2779.525760	17.533939	-0.054111	2.913921
281.830669	2771.476466	17.538944	-0.054058	2.910015
281.891749	2763.510058	17.543949	-0.054064	2.906160
281.954783	2755.516656	17.548954	-0.054071	2.902287
282.011468	2747.541017	17.553959	-0.054076	2.898417
281.988067	2739.586790	17.558963	-0.054067	2.894549
282.013103	2731.581448	17.563968	-0.054066	2.890652
281.764169	2723.647395	17.568973	-0.054014	2.886771
281.670634	2715.656369	17.573978	-0.053992	2.882864
281.774741	2707.679724	17.578983	-0.054006	2.878971
281.620243	2699.718470	17.583987	-0.053972	2.875065
281.542890	2691.699661	17.588992	-0.053952	2.871130
281.671361	2683.708235	17.593997	-0.053971	2.867214
281.617937	2675.731567	17.599002	-0.053956	2.863291
281.379178	2667.787331	17.604007	-0.053906	2.859367
281.281556	2659.818612	17.609011	-0.053883	2.855434
281.291460	2651.810237	17.614016	-0.053879	2.851482
281.449075	2643.830355	17.619021	-0.053903	2.847547
281.132931	2635.877223	17.624026	-0.053839	2.843593
281.279491	2627.874678	17.629031	-0.053861	2.839635
281.158126	2619.938156	17.634035	-0.053834	2.835689
281.114380	2611.905994	17.639040	-0.053820	2.831694
281.300307	2603.906026	17.644045	-0.053850	2.827723
281.286793	2595.911795	17.649050	-0.053842	2.823738
281.129911	2587.980254	17.654055	-0.053807	2.819770
281.119535	2580.025081	17.659059	-0.053800	2.815793
280.951411	2572.004510	17.664064	-0.053764	2.811769
280.982182	2564.037384	17.669069	-0.053764	2.807777
280.884248	2556.045423	17.674074	-0.053741	2.803760
281.127328	2548.079020	17.679079	-0.053781	2.799769
280.870436	2540.158041	17.684083	-0.053728	2.795767
280.895275	2532.126837	17.689088	-0.053727	2.791719
281.181488	2524.119611	17.694093	-0.053775	2.787694
281.027973	2516.161881	17.699098	-0.053741	2.783661
280.923378	2508.216856	17.704103	-0.053717	2.779632
280.882852	2500.260563	17.709107	-0.053704	2.775596
280.825382	2492.249650	17.714112	-0.053688	2.771524
280.804018	2484.275152	17.719117	-0.053679	2.767467
280.627726	2476.305377	17.724122	-0.053641	2.763398
280.543166	2468.369714	17.729127	-0.053620	2.759345
280.705654	2460.382542	17.734131	-0.053645	2.755275
280.609624	2452.303325	17.739136	-0.053622	2.751136
280.632681	2444.331892	17.744141	-0.053621	2.747054
280.392764	2436.381442	17.749146	-0.053571	2.742960
280.281179	2428.435110	17.754151	-0.053545	2.738870
280.343206	2420.467424	17.759155	-0.053551	2.734773
280.540560	2412.436274	17.764160	-0.053583	2.730646
280.274145	2404.504273	17.769165	-0.053528	2.726535
280.115591	2396.549223	17.774170	-0.053493	2.722413
280.348110	2388.575974	17.779175	-0.053531	2.718299
280.278329	2380.617054	17.784179	-0.053513	2.714167
280.219457	2372.580083	17.789184	-0.053497	2.709990
280.059484	2364.648612	17.794189	-0.053462	2.705854
280.161307	2356.658430	17.799194	-0.053475	2.701698
279.986980	2348.703494	17.804199	-0.053438	2.697537
279.946872	2340.740003	17.809203	-0.053425	2.693373
279.780471	2332.736117	17.814208	-0.053389	2.689174
279.856132	2324.780476	17.819213	-0.053398	2.685008
279.648640	2316.825022	17.824218	-0.053354	2.680819
279.814924	2308.853468	17.829223	-0.053380	2.676638
279.876104	2300.858448	17.834227	-0.053386	2.672431
279.713867	2292.855215	17.839232	-0.053350	2.668199
279.837775	2284.894905	17.844237	-0.053368	2.664002
279.545734	2276.926424	17.849242	-0.053309	2.659766
279.611832	2268.978294	17.854247	-0.053316	2.655558
279.496499	2260.994971	17.859251	-0.053289	2.651313
279.553560	2252.994002	17.864256	-0.053294	2.647063
279.467976	2245.059073	17.869261	-0.053273	2.642831
279.370016	2237.097188	17.874266	-0.053250	2.638578
279.610351	2229.113874	17.879271	-0.053289	2.634329
279.713692	2221.094305	17.884275	-0.053303	2.630044
279.368597	2213.164035	17.889280	-0.053234	2.625771
279.308010	2205.212869	17.894285	-0.053217	2.621498
279.293793	2197.232412	17.899290	-0.053209	2.617206
279.318460	2189.257624	17.904295	-0.053209	2.612912
279.268446	2181.287278	17.909299	-0.053194	2.608608
279.029358	2173.339484	17.914304	-0.053145	2.604297
279.137348	2165.383652	17.919309	-0.053159	2.599998
279.166758	2157.408717	17.924314	-0.053160	2.595676
279.111949	2149.266310	17.929319	-0.053144	2.591250
278.917422	2141.304403	17.934323	-0.053103	2.586905
278.596248	2133.381302	17.939328	-0.053038	2.582565
278.885487	2125.422794	17.944333	-0.053086	2.578240
278.800489	2117.470033	17.949338	-0.053065	2.573886
278.643423	2109.508812	17.954343	-0.053031	2.569514
278.453140	2101.584464	17.959347	-0.052990	2.565153
278.654338	2093.607797	17.964352	-0.053022	2.560783
278.673495	2085.657733	17.969357	-0.053021	2.556408
278.364052	2077.683705	17.974362	-0.052958	2.551989
278.400839	2069.704304	17.979367	-0.052960	2.547583
278.738099	2061.693733	17.984371	-0.053017	2.543174
278.488692	2053.760254	17.989376	-0.052965	2.538758
278.424767	2045.827193	17.994381	-0.052948	2.534348
278.515304	2037.812840	17.999386	-0.052960	2.529896
278.542218	2029.869644	18.004391	-0.052960	2.525472
278.448522	2021.932041	18.009395	-0.052937	2.521034
278.347726	2013.972008	18.014400	-0.052913	2.516575
278.615104	2005.957144	18.019405	-0.052958	2.512104
278.235598	1998.007896	18.024410	-0.052882	2.507615
277.939447	1990.083732	18.029415	-0.052821	2.503138
278.162446	1982.105844	18.034419	-0.052858	2.498661
278.095235	1974.131236	18.039424	-0.052840	2.494156
277.999198	1966.158799	18.044429	-0.052817	2.489642
277.973840	1958.187584	18.049434	-0.052807	2.485126
278.129918	1950.212821	18.054439	-0.052831	2.480613
277.957429	1942.294070	18.059443	-0.052793	2.476099
277.840160	1934.302698	18.064448	-0.052766	2.471540
278.012209	1926.330527	18.069453	-0.052793	2.467005
277.852789	1918.383153	18.074458	-0.052758	2.462451
277.876322	1910.433193	18.079463	-0.052757	2.457901
277.846877	1902.469255	18.084467	-0.052747	2.453330
277.522788	1894.503176	18.089472	-0.052681	2.448727
277.542005	1886.558381	18.094477	-0.052680	2.444154
277.531665	1878.592855	18.099482	-0.052672	2.439558
277.682481	1870.617068	18.104487	-0.052695	2.434959
277.620241	1862.576889	18.109491	-0.052678	2.430299
277.573512	1854.611132	18.114496	-0.052665	2.425673
277.468769	1846.708505	18.119501	-0.052640	2.421072
277.260389	1838.767213	18.124506	-0.052596	2.416430
277.184515	1830.805017	18.129511	-0.052576	2.411778
277.355680	1822.816336	18.134515	-0.052603	2.407121
277.116200	1814.883255	18.139520	-0.052553	2.402455
276.942513	1806.970250	18.144525	-0.052516	2.397797
277.136430	1798.962951	18.149530	-0.052547	2.393103
277.232543	1790.979796	18.154535	-0.052559	2.388407
277.293984	1783.015062	18.159539	-0.052566	2.383709
276.995535	1775.096017	18.164544	-0.052505	2.379001
277.061314	1767.149217	18.169549	-0.052512	2.374296
277.043689	1759.161584	18.174554	-0.052503	2.369550
276.991300	1751.211403	18.179559	-0.052488	2.364815
276.820859	1743.299096	18.184563	-0.052451	2.360083
276.755261	1735.335106	18.189568	-0.052434	2.355319
276.946746	1727.326470	18.194573	-0.052464	2.350540
276.851041	1719.364019	18.199578	-0.052441	2.345755
276.786614	1711.432304	18.204583	-0.052424	2.340982
276.808084	1703.487797	18.209587	-0.052423	2.336198
276.617684	1695.529178	18.214592	-0.052382	2.331378
276.601050	1687.580495	18.219597	-0.052374	2.326568
276.551728	1679.629550	18.224602	-0.052360	2.321745
276.422641	1671.698593	18.229607	-0.052330	2.316917
276.396717	1663.731712	18.234611	-0.052320	2.312065
276.407326	1655.746647	18.239616	-0.052317	2.307196
276.355738	1647.829296	18.244621	-0.052302	2.302352
276.313665	1639.865716	18.249626	-0.052289	2.297470
276.386557	1631.907594	18.254631	-0.052298	2.292591
276.262276	1623.950907	18.259635	-0.052269	2.287686
276.122618	1616.023595	18.264640	-0.052238	2.282787
276.397305	1608.068554	18.269645	-0.052284	2.277896
276.107147	1600.108494	18.274650	-0.052225	2.272943
275.969489	1592.118977	18.279655	-0.052194	2.267974
276.003839	1584.169599	18.284659	-0.052195	2.263033
275.901427	1576.221998	18.289664	-0.052171	2.258071
275.938217	1568.279316	18.294669	-0.052172	2.253114
275.926689	1560.308740	18.299674	-0.052165	2.248123
275.755905	1552.389488	18.304679	-0.052128	2.243140
275.856295	1544.449345	18.309683	-0.052141	2.238156
275.656743	1536.523444	18.314688	-0.052099	2.233144
275.727895	1528.546222	18.319693	-0.052107	2.228112
275.585029	1520.607345	18.324698	-0.052075	2.223074
275.538419	1512.674762	18.329703	-0.052061	2.218037
275.589233	1504.729606	18.334707	-0.052066	2.212989
275.394486	1496.770788	18.339712	-0.052024	2.207899
275.547453	1488.831481	18.344717	-0.052047	2.202841
275.451771	1480.899836	18.349722	-0.052024	2.197754
275.492185	1472.924619	18.354727	-0.052027	2.192639
275.301382	1464.998987	18.359731	-0.051986	2.187523
275.090796	1457.074265	18.364736	-0.051942	2.182394
275.208866	1449.120230	18.369741	-0.051958	2.177264
275.131032	1441.171760	18.374746	-0.051939	2.172107
274.927569	1433.240389	18.379751	-0.051896	2.166938
274.959764	1425.300491	18.384755	-0.051896	2.161772
274.997571	1417.351251	18.389760	-0.051898	2.156589
274.976812	1409.406084	18.394765	-0.051889	2.151390
274.884590	1401.466323	18.399770	-0.051867	2.146175
274.921614	1393.531430	18.404775	-0.051869	2.140964
274.970404	1385.595668	18.409779	-0.051872	2.135739
274.889734	1377.641680	18.414784	-0.051852	2.130478
274.699221	1369.738011	18.419789	-0.051811	2.125227
274.681233	1361.801674	18.424794	-0.051803	2.119957
274.731867	1353.870485	18.429799	-0.051807	2.114685
274.668883	1345.863244	18.434803	-0.051790	2.109337
274.670212	1337.917158	18.439808	-0.051785	2.104023
274.553321	1330.019632	18.444813	-0.051758	2.098716
274.600605	1322.072427	18.449818	-0.051762	2.093379
274.629176	1314.120159	18.454823	-0.051762	2.088023
274.646002	1306.199881	18.459827	-0.051760	2.082673
274.312656	1298.318657	18.464832	-0.051693	2.077302
274.323845	1290.377314	18.469837	-0.051690	2.071909
274.444873	1282.386325	18.474842	-0.051707	2.066480
274.187840	1274.505938	18.479847	-0.051654	2.061075
274.226825	1266.587151	18.484851	-0.051656	2.055658
274.140864	1258.632754	18.489856	-0.051635	2.050190
274.272669	1250.706417	18.494861	-0.051654	2.044749
274.030471	1242.816670	18.499866	-0.051604	2.039281
274.001647	1234.892535	18.504871	-0.051593	2.033796
273.939846	1226.929016	18.509875	-0.051576	2.028265
273.761156	1219.000891	18.514880	-0.051538	2.022732
273.952660	1211.076573	18.519885	-0.051568	2.017224
273.928654	1203.130694	18.524890	-0.051559	2.011664
273.899438	1195.191546	18.529895	-0.051548	2.006092
273.845974	1187.301315	18.534899	-0.051533	2.000537
273.688488	1179.400050	18.539904	-0.051499	1.994948
273.674551	1171.459364	18.544909	-0.051491	1.989330
273.564449	1163.538257	18.549914	-0.051465	1.983701
273.721154	1155.608717	18.554919	-0.051489	1.978077
273.649999	1147.698195	18.559923	-0.051471	1.972427
273.479288	1139.773163	18.564928	-0.051434	1.966739
273.597426	1131.852085	18.569933	-0.051450	1.961069
273.528611	1123.953841	18.574938	-0.051432	1.955378
273.296572	1115.998330	18.579943	-0.051384	1.949612
273.284400	1108.077010	18.584947	-0.051377	1.943877
273.276200	1100.151394	18.589952	-0.051370	1.938123
273.207211	1092.258012	18.594957	-0.051352	1.932368
273.158530	1084.326201	18.599962	-0.051338	1.926571
273.110973	1076.432149	18.604967	-0.051324	1.920783
273.173067	1068.512872	18.609971	-0.051330	1.914972
273.063897	1060.587409	18.614976	-0.051304	1.909119
272.862577	1052.710174	18.619981	-0.051262	1.903274
272.764671	1044.799973	18.624986	-0.051238	1.897398
272.674047	1036.882836	18.629991	-0.051216	1.891499
272.645603	1028.985164	18.634995	-0.051206	1.885603
272.689903	1021.067165	18.640000	-0.051209	1.879682
272.740827	1013.165352	18.645005	-0.051213	1.873755
272.444131	1005.254605	18.650010	-0.051153	1.867762
272.406367	997.347227	18.655015	-0.051140	1.861783
272.620236	989.418116	18.660019	-0.051175	1.855797
272.537205	981.494677	18.665024	-0.051154	1.849761
272.308863	973.643114	18.670029	-0.051107	1.843744
272.392387	965.731181	18.675034	-0.051117	1.837697
272.291137	957.833409	18.680039	-0.051093	1.831619
272.528413	949.893406	18.685043	-0.051132	1.825529
272.059530	942.060878	18.690048	-0.051040	1.819417
272.205853	934.148455	18.695053	-0.051062	1.813296
272.143620	926.233741	18.700058	-0.051045	1.807128
272.064936	918.355791	18.705063	-0.051025	1.800965
272.122667	910.470383	18.710067	-0.051031	1.794792
272.009417	902.513106	18.715072	-0.051004	1.788520
272.142357	894.614479	18.720077	-0.051024	1.782302
272.145228	886.729233	18.725082	-0.051019	1.776057
272.118800	878.831728	18.730087	-0.051009	1.769777
272.031454	870.973487	18.735091	-0.050988	1.763498
271.707632	863.133059	18.740096	-0.050922	1.757181
271.890363	855.215368	18.745101	-0.050951	1.750844
271.829160	847.320800	18.750106	-0.050935	1.744470
271.593872	839.484857	18.755111	-0.050886	1.738099
271.511110	831.596928	18.760115	-0.050865	1.731682
271.495331	823.703289	18.765120	-0.050857	1.725244
271.497954	815.844178	18.770125	-0.050852	1.718814
271.465894	807.953872	18.775130	-0.050841	1.712328
271.273922	800.077626	18.780135	-0.050800	1.705809
271.234209	792.218332	18.785139	-0.050788	1.699299
271.287378	784.318965	18.790144	-0.050792	1.692743
271.464233	776.418391	18.795149	-0.050820	1.686176
271.301965	768.573772	18.800154	-0.050785	1.679586
271.037550	760.743992	18.805159	-0.050731	1.672969
271.099781	752.845194	18.810163	-0.050737	1.666310
270.892410	745.004872	18.815168	-0.050693	1.659639
270.861713	737.152006	18.820173	-0.050682	1.652953
270.728818	729.276038	18.825178	-0.050652	1.646207
270.971883	721.381010	18.830183	-0.050692	1.639468
270.888791	713.542529	18.835187	-0.050672	1.632705
270.593456	705.661870	18.840192	-0.050612	1.625848
270.858463	697.778108	18.845197	-0.050656	1.619037
270.733949	689.940295	18.850202	-0.050628	1.612183
270.380280	682.124268	18.855207	-0.050557	1.605287
270.631716	674.255396	18.860211	-0.050598	1.598400
270.533327	666.401073	18.865216	-0.050575	1.591446
270.549677	658.549477	18.870221	-0.050573	1.584481
270.431111	650.726276	18.875226	-0.050545	1.577490
270.407507	642.875163	18.880231	-0.050536	1.570457
270.382618	635.046906	18.885235	-0.050526	1.563413
270.023088	627.266284	18.890240	-0.050454	1.556332
270.237892	619.369532	18.895245	-0.050489	1.549196
270.132615	611.536987	18.900250	-0.050464	1.542039
269.875823	603.752172	18.905255	-0.050411	1.534870
269.923716	595.900612	18.910259	-0.050415	1.527651
269.989375	588.048103	18.915264	-0.050422	1.520400
269.898350	580.252881	18.920269	-0.050400	1.513143
269.524559	572.452442	18.925274	-0.050325	1.505804
269.633021	564.616128	18.930279	-0.050340	1.498469
269.746979	556.781721	18.935283	-0.050356	1.491100
269.350927	549.016512	18.940288	-0.050278	1.483681
269.413797	541.204541	18.945293	-0.050284	1.476252
269.553879	533.308917	18.950298	-0.050305	1.468717
269.248376	525.541591	18.955303	-0.050243	1.461197
269.301619	517.733327	18.960307	-0.050248	1.453655
269.015872	509.950410	18.965312	-0.050190	1.446044
268.986873	502.173579	18.970317	-0.050179	1.438440
268.871750	494.369594	18.975322	-0.050153	1.430755
268.950061	486.554977	18.980327	-0.050162	1.423049
269.009495	478.766938	18.985331	-0.050168	1.415325
268.958818	470.971004	18.990336	-0.050153	1.407532
269.061622	463.187018	18.995341	-0.050168	1.399734
268.937366	455.425086	19.000346	-0.050139	1.391876
268.711836	447.660687	19.005351	-0.050092	1.383954
268.514810	439.926271	19.010355	-0.050050	1.376021
268.390815	432.149726	19.015360	-0.050022	1.368012
268.541700	424.363607	19.020365	-0.050045	1.359993
268.222165	416.645698	19.025370	-0.049981	1.351916
268.204768	408.877607	19.030375	-0.049972	1.343790
268.290465	401.108298	19.035379	-0.049983	1.335632
267.952364	393.387885	19.040384	-0.049915	1.327400
268.130334	385.625622	19.045389	-0.049943	1.319165
268.023006	377.810111	19.050394	-0.049918	1.310769
267.765937	370.059792	19.055399	-0.049865	1.302362
268.005013	362.301523	19.060403	-0.049905	1.293983
267.805265	354.596239	19.065408	-0.049862	1.285526
267.847325	346.891697	19.070413	-0.049865	1.277059
267.539497	339.212252	19.075418	-0.049803	1.268498
267.566645	331.494243	19.080423	-0.049803	1.259898
267.692496	323.772100	19.085427	-0.049821	1.251254
267.360198	316.122894	19.090432	-0.049754	1.242544
267.344217	308.429086	19.095437	-0.049746	1.233783
267.339010	300.710998	19.100442	-0.049740	1.224934
267.193691	293.053763	19.105447	-0.049708	1.216063
267.113578	285.382314	19.110451	-0.049688	1.207123
267.278285	277.681421	19.115456	-0.049714	1.198130
267.382340	270.004064	19.120461	-0.049728	1.189086
267.107085	262.389757	19.125466	-0.049672	1.179970
266.920928	254.761018	19.130471	-0.049632	1.170784
267.095631	247.093495	19.135475	-0.049660	1.161553
266.913774	239.471264	19.140480	-0.049621	1.152229
266.924081	231.819333	19.145485	-0.049618	1.142833
266.983421	224.177833	19.150490	-0.049624	1.133382
266.647519	216.614951	19.155495	-0.049556	1.123865
266.658722	209.013985	19.160499	-0.049553	1.114294
266.648741	201.395040	19.165504	-0.049547	1.104613
266.710510	193.807878	19.170509	-0.049553	1.094903
266.603926	186.236705	19.175514	-0.049528	1.085088
266.468597	178.696839	19.180519	-0.049498	1.075219
266.450665	171.126451	19.185523	-0.049490	1.065245
266.321869	163.591199	19.190528	-0.049461	1.055198
266.193026	156.062120	19.195533	-0.049432	1.045063
266.213052	148.537370	19.200538	-0.049431	1.034869
266.012207	141.040809	19.205543	-0.049389	1.024560
266.032659	133.536706	19.210547	-0.049387	1.014188
265.874817	126.051927	19.215552	-0.049353	1.003694
265.805467	118.583648	19.220557	-0.049335	0.993133
265.510903	111.126530	19.225562	-0.049276	0.982419
265.236169	103.707481	19.230567	-0.049220	0.971647
265.542879	96.206524	19.235571	-0.049272	0.960782
265.496937	88.779517	19.240576	-0.049258	0.949812
265.340922	81.393753	19.245581	-0.049224	0.938746
265.275575	74.001845	19.250586	-0.049207	0.927564
265.157724	66.648072	19.255591	-0.049181	0.916289
264.919798	59.543533	19.260595	-0.049132	0.905229