Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
0.601063	-0.015097	0.000000	-0.000023	0.721136
0.604078	-0.022358	0.005005	-0.000024	0.721123
0.648313	-0.026008	0.010010	-0.000032	0.721131
0.688057	-0.034929	0.015014	-0.000040	0.721128
0.505010	-0.004494	0.020019	-0.000006	0.721124
0.518193	-0.003288	0.025024	-0.000008	0.721131
0.563635	-0.048774	0.030029	-0.000017	0.721057
0.668043	-0.156681	0.035034	-0.000036	0.720881
0.594499	-0.145031	0.040038	-0.000022	0.720879
0.402160	-0.112384	0.045043	0.000014	0.720875
0.559049	-0.135898	0.050048	-0.000016	0.720884
0.601891	-0.149733	0.055053	-0.000024	0.720872
0.748214	-0.171049	0.060058	-0.000051	0.720881
0.542320	-0.136147	0.065062	-0.000013	0.720878
0.619072	-0.150428	0.070067	-0.000027	0.720877
0.714629	-0.165321	0.075072	-0.000045	0.720881
0.593657	-0.232556	0.080077	-0.000022	0.720706
0.416869	-0.285468	0.085082	0.000011	0.720540
0.674282	-0.331842	0.090086	-0.000037	0.720539
0.613631	-0.323200	0.095091	-0.000026	0.720535
0.810613	-0.353064	0.100096	-0.000063	0.720545
0.882490	-0.370798	0.105101	-0.000076	0.720536
0.868739	-0.470164	0.110106	-0.000073	0.720335
0.443889	-0.451237	0.115110	0.000006	0.720224
0.732323	-0.504642	0.120115	-0.000048	0.720220
0.751959	-0.503916	0.125120	-0.000052	0.720228
0.671516	-0.494642	0.130125	-0.000037	0.720218
0.659117	-0.648871	0.135130	-0.000034	0.719910
0.524568	-0.629206	0.140134	-0.000009	0.719901
0.524595	-0.630576	0.145139	-0.000009	0.719899
0.608188	-0.641916	0.150144	-0.000025	0.719906
0.659107	-0.787873	0.155149	-0.000034	0.719636
0.659926	-0.804113	0.160154	-0.000034	0.719604
0.480525	-0.773171	0.165158	-0.000001	0.719602
0.512812	-0.820115	0.170163	-0.000007	0.719521
0.798556	-0.996818	0.175168	-0.000060	0.719273
0.425078	-0.935901	0.180173	0.000009	0.719262
0.565665	-0.956683	0.185178	-0.000017	0.719271
0.675246	-1.124480	0.190182	-0.000037	0.718978
0.320251	-1.070807	0.195187	0.000029	0.718959
0.367070	-1.074614	0.200192	0.000020	0.718968
0.311758	-1.201829	0.205197	0.000030	0.718698
0.411464	-1.245466	0.210202	0.000012	0.718647
0.370909	-1.239052	0.215206	0.000019	0.718645
0.591659	-1.411223	0.220211	-0.000022	0.718383
0.584688	-1.423083	0.225216	-0.000020	0.718357
0.180219	-1.386989	0.230221	0.000055	0.718286
0.293374	-1.541589	0.235226	0.000034	0.718021
0.478596	-1.574598	0.240230	-0.000000	0.718021
0.259097	-1.630049	0.245235	0.000040	0.717834
0.443880	-1.724748	0.250240	0.000006	0.717712
0.258413	-1.712976	0.255245	0.000041	0.717670
0.393846	-1.881772	0.260250	0.000015	0.717384
0.308978	-1.868174	0.265254	0.000031	0.717381
0.319692	-1.984038	0.270259	0.000029	0.717156
0.333363	-2.021451	0.275264	0.000027	0.717086
-0.009299	-2.039848	0.280269	0.000091	0.716929
0.013111	-2.131025	0.285274	0.000086	0.716757
0.068175	-2.170902	0.290278	0.000076	0.716697
-0.207328	-2.247538	0.295283	0.000127	0.716449
-0.434065	-2.203541	0.300288	0.000170	0.716456
-0.656191	-2.316043	0.305293	0.000211	0.716155
-2.772067	-1.948329	0.310298	0.000605	0.716136
-2.091979	-2.087619	0.315302	0.000478	0.716101
-2.717833	-2.088222	0.320307	0.000595	0.715878
-3.205078	-1.996047	0.325312	0.000685	0.715889
-2.999978	-2.039298	0.330317	0.000647	0.715876
-3.343802	-2.134749	0.335322	0.000711	0.715565
-4.031309	-2.022647	0.340326	0.000839	0.715545
-4.274725	-1.982373	0.345331	0.000884	0.715539
-3.669958	-2.145511	0.350336	0.000772	0.715429
-5.009090	-2.009015	0.355341	0.001021	0.715227
-5.069247	-1.996191	0.360346	0.001032	0.715231
-4.966530	-2.014194	0.365350	0.001013	0.715231
-5.042421	-2.047829	0.370355	0.001027	0.715138
-5.939984	-2.000804	0.375360	0.001194	0.714914
-5.711838	-2.047130	0.380365	0.001152	0.714903
-5.708695	-2.044129	0.385370	0.001151	0.714910
-5.783962	-2.030385	0.390374	0.001165	0.714910
-6.249542	-2.069990	0.395379	0.001252	0.714667
-6.712701	-2.016234	0.400384	0.001338	0.714610
-6.562919	-2.048125	0.405389	0.001310	0.714600
-6.540200	-2.048968	0.410394	0.001306	0.714606
-6.857035	-1.992422	0.415398	0.001365	0.714607
-7.199600	-2.083635	0.420403	0.001429	0.714304
-7.659907	-2.013945	0.425408	0.001514	0.714280
-8.089586	-1.941852	0.430413	0.001594	0.714271
-7.650536	-2.017615	0.435418	0.001513	0.714276
-7.582695	-2.028934	0.440422	0.001500	0.714278
-8.120163	-1.971467	0.445427	0.001600	0.714201
-8.295221	-2.055356	0.450432	0.001633	0.713973
-8.601243	-2.006312	0.455437	0.001690	0.713962
-8.950284	-1.939980	0.460442	0.001755	0.713970
-8.355839	-2.047006	0.465446	0.001644	0.713968
-8.416279	-2.040734	0.470451	0.001655	0.713959
-8.583554	-2.070093	0.475456	0.001686	0.713842
-9.483077	-2.008516	0.480461	0.001854	0.713646
-9.328471	-2.033096	0.485466	0.001825	0.713651
-9.339877	-2.032181	0.490470	0.001827	0.713649
-9.696573	-1.969983	0.495475	0.001893	0.713647
-9.096288	-2.072084	0.500480	0.001782	0.713656
-9.267626	-2.093313	0.505485	0.001814	0.713553
-10.283088	-2.009739	0.510490	0.002003	0.713360
-10.327587	-2.001358	0.515494	0.002011	0.713361
-10.529449	-1.967765	0.520499	0.002048	0.713356
-10.150386	-2.032025	0.525504	0.001978	0.713363
-10.367574	-1.997663	0.530509	0.002018	0.713354
-10.506208	-1.969920	0.535514	0.002044	0.713360
-10.359724	-2.140218	0.540518	0.002017	0.713073
-11.506210	-1.963182	0.545523	0.002230	0.713019
-11.482385	-1.962739	0.550528	0.002226	0.713029
-11.105502	-2.034183	0.555533	0.002156	0.713020
-11.537012	-1.955591	0.560538	0.002236	0.713023
-11.540068	-1.954438	0.565542	0.002236	0.713025
-11.284955	-2.005244	0.570547	0.002189	0.713014
-11.737248	-2.071369	0.575552	0.002273	0.712722
-12.589444	-1.930286	0.580557	0.002432	0.712701
-12.388902	-1.963096	0.585562	0.002394	0.712707
-11.826206	-2.062041	0.590566	0.002290	0.712709
-12.534641	-1.939870	0.595571	0.002421	0.712701
-12.242805	-1.986673	0.600576	0.002367	0.712712
-12.000752	-2.033818	0.605581	0.002322	0.712704
-12.864085	-2.029260	0.610586	0.002483	0.712406
-13.346064	-1.953194	0.615590	0.002572	0.712387
-13.370289	-1.952148	0.620595	0.002577	0.712380
-12.913781	-2.028728	0.625600	0.002492	0.712390
-13.342409	-1.956565	0.630605	0.002572	0.712382
-13.344227	-1.955789	0.635610	0.002572	0.712383
-12.891109	-2.036780	0.640614	0.002488	0.712382
-13.397491	-2.045182	0.645619	0.002582	0.712186
-14.297877	-1.932434	0.650624	0.002750	0.712091
-13.881310	-2.010439	0.655629	0.002672	0.712083
-13.954515	-1.995612	0.660634	0.002686	0.712087
-14.071578	-1.972460	0.665638	0.002707	0.712091
-13.834150	-2.020111	0.670643	0.002663	0.712081
-13.870238	-2.009116	0.675648	0.002670	0.712090
-14.668325	-1.988636	0.680653	0.002818	0.711847
-15.209835	-1.937264	0.685658	0.002919	0.711757
-14.770122	-2.015048	0.690662	0.002837	0.711759
-15.122397	-1.954799	0.695667	0.002903	0.711754
-14.872849	-1.993921	0.700672	0.002856	0.711764
-14.498132	-2.065017	0.705677	0.002787	0.711756
-14.799128	-2.010774	0.710682	0.002843	0.711757
-15.293788	-2.017648	0.715686	0.002935	0.711567
-16.277353	-1.901532	0.720691	0.003118	0.711450
-15.538034	-2.028518	0.725696	0.002980	0.711459
-15.778986	-1.990609	0.730701	0.003025	0.711449
-16.033549	-1.943700	0.735706	0.003072	0.711452
-15.688452	-2.003843	0.740710	0.003008	0.711455
-16.046874	-1.944258	0.745715	0.003075	0.711446
-15.850727	-2.020313	0.750720	0.003038	0.711364
-16.733064	-1.978229	0.755725	0.003203	0.711135
-16.502970	-2.018702	0.760730	0.003160	0.711136
-16.803011	-1.964432	0.765734	0.003216	0.711137
-16.777399	-1.972886	0.770739	0.003211	0.711130
-16.124956	-2.084436	0.775744	0.003089	0.711139
-16.900509	-1.951532	0.780749	0.003234	0.711129
-16.927579	-1.991780	0.785754	0.003239	0.711039
-17.299428	-2.008822	0.790758	0.003308	0.710873
-17.460335	-1.985679	0.795763	0.003338	0.710861
-17.520046	-1.969270	0.800768	0.003349	0.710873
-17.362343	-2.001809	0.805773	0.003320	0.710864
-17.133377	-2.041261	0.810778	0.003277	0.710867
-17.440633	-1.984689	0.815782	0.003334	0.710871
-17.889355	-2.033270	0.820787	0.003418	0.710614
-18.229317	-2.013232	0.825792	0.003481	0.710533
-18.360862	-1.991840	0.830797	0.003505	0.710529
-18.211167	-2.018378	0.835802	0.003478	0.710529
-18.304597	-1.999754	0.840806	0.003495	0.710533
-18.314238	-2.000985	0.845811	0.003497	0.710527
-18.245615	-2.013114	0.850816	0.003484	0.710528
-18.763928	-2.078446	0.855821	0.003580	0.710213
-19.045212	-2.027399	0.860826	0.003633	0.710215
-19.215472	-1.995513	0.865830	0.003664	0.710218
-19.084182	-2.022991	0.870835	0.003640	0.710210
-18.957330	-2.040732	0.875840	0.003616	0.710219
-19.240217	-1.995064	0.880845	0.003669	0.710210
-19.366690	-2.025855	0.885850	0.003693	0.710103
-19.828439	-2.048347	0.890854	0.003779	0.709894
-19.721612	-2.071151	0.895859	0.003759	0.709886
-20.334699	-1.958122	0.900864	0.003873	0.709894
-20.232315	-1.980915	0.905869	0.003854	0.709885
-20.114379	-2.001014	0.910874	0.003832	0.709887
-20.225983	-1.978839	0.915878	0.003852	0.709891
-20.368056	-1.980163	0.920883	0.003879	0.709838
-20.575967	-2.064201	0.925888	0.003918	0.709596
-20.748455	-2.037811	0.930893	0.003950	0.709587
-21.346111	-1.929365	0.935898	0.004061	0.709591
-20.814442	-2.022380	0.940902	0.003962	0.709595
-21.019812	-1.990168	0.945907	0.004000	0.709586
-21.310226	-1.934488	0.950912	0.004054	0.709594
-21.165019	-1.963663	0.955917	0.004027	0.709587
-21.820527	-2.009661	0.960922	0.004149	0.709262
-22.041466	-1.968353	0.965926	0.004190	0.709266
-22.391721	-1.908678	0.970931	0.004255	0.709260
-21.969572	-1.982411	0.975936	0.004177	0.709263
-22.153180	-1.953451	0.980941	0.004211	0.709256
-22.581933	-1.875769	0.985946	0.004291	0.709258
-21.770609	-2.018355	0.990950	0.004140	0.709262
-22.040712	-2.007989	0.995955	0.004190	0.709187
-22.925178	-1.965716	1.000960	0.004355	0.708956
-22.668949	-2.013623	1.005965	0.004307	0.708951
-23.219751	-1.916839	1.010970	0.004409	0.708949
-22.731529	-2.000050	1.015974	0.004319	0.708956
-23.206456	-1.920765	1.020979	0.004407	0.708946
-23.064613	-1.943062	1.025984	0.004381	0.708952
-22.671488	-2.015835	1.030989	0.004307	0.708946
-23.566375	-2.004592	1.035994	0.004474	0.708649
-23.614777	-2.001673	1.040998	0.004483	0.708638
-23.930795	-1.951291	1.046003	0.004542	0.708626
-23.566055	-2.012381	1.051008	0.004474	0.708634
-23.687450	-1.992282	1.056013	0.004496	0.708631
-23.959275	-1.944438	1.061018	0.004547	0.708630
-23.742107	-1.979304	1.066022	0.004507	0.708638
-24.539249	-1.969440	1.071027	0.004655	0.708373
-24.663656	-1.958114	1.076032	0.004678	0.708351
-24.346385	-2.020951	1.081037	0.004619	0.708339
-24.722246	-1.951019	1.086042	0.004689	0.708344
-24.726623	-1.947608	1.091046	0.004690	0.708350
-24.634787	-1.967773	1.096051	0.004673	0.708342
-24.420513	-2.003800	1.101056	0.004633	0.708347
-25.229227	-2.015137	1.106061	0.004783	0.708035
-25.660586	-1.954194	1.111066	0.004864	0.708003
-25.490106	-1.981756	1.116070	0.004832	0.708009
-25.601262	-1.964376	1.121075	0.004852	0.708004
-25.462680	-1.984812	1.126080	0.004827	0.708013
-25.464304	-1.987111	1.131085	0.004827	0.708007
-25.590123	-1.965287	1.136090	0.004850	0.708006
-25.651975	-2.074521	1.141094	0.004862	0.707765
-26.266660	-2.002687	1.146099	0.004976	0.707689
-26.220445	-2.005184	1.151104	0.004968	0.707701
-26.359967	-1.982940	1.156109	0.004994	0.707696
-26.813432	-1.902327	1.161114	0.005078	0.707695
-26.442685	-1.965392	1.166118	0.005009	0.707701
-26.685717	-1.928163	1.171123	0.005054	0.707689
-26.796699	-2.026832	1.176128	0.005075	0.707452
-27.420940	-1.956658	1.181133	0.005191	0.707369
-27.748049	-1.898838	1.186138	0.005252	0.707368
-27.387664	-1.961148	1.191142	0.005185	0.707372
-27.467978	-1.951168	1.196147	0.005200	0.707364
-27.275873	-1.978932	1.201152	0.005164	0.707377
-27.467347	-1.947466	1.206157	0.005200	0.707371
-27.518464	-1.982944	1.211162	0.005209	0.707282
-28.182615	-1.964279	1.216166	0.005333	0.707082
-28.321318	-1.943967	1.221171	0.005359	0.707073
-28.626535	-1.886315	1.226176	0.005415	0.707080
-28.215726	-1.963019	1.231181	0.005339	0.707073
-28.234699	-1.959733	1.236186	0.005342	0.707072
-28.425518	-1.922472	1.241190	0.005378	0.707079
-28.163571	-1.974081	1.246195	0.005329	0.707069
-28.559878	-2.063442	1.251200	0.005403	0.706748
-29.390250	-1.917736	1.256205	0.005557	0.706743
-29.600497	-1.878995	1.261210	0.005597	0.706746
-28.883748	-2.003434	1.266214	0.005463	0.706753
-29.377184	-1.919304	1.271219	0.005555	0.706745
-29.274871	-1.933985	1.276224	0.005536	0.706752
-29.058179	-1.974999	1.281229	0.005496	0.706747
-29.501749	-2.023074	1.286234	0.005578	0.706492
-30.071778	-1.945835	1.291238	0.005684	0.706443
-30.087503	-1.947945	1.296243	0.005687	0.706433
-30.004385	-1.959516	1.301248	0.005672	0.706440
-30.079738	-1.945559	1.306253	0.005686	0.706441
-29.940793	-1.970811	1.311258	0.005660	0.706440
-29.665378	-2.018214	1.316262	0.005609	0.706443
-30.790364	-1.979044	1.321267	0.005818	0.706119
-31.096880	-1.920579	1.326272	0.005875	0.706127
-30.840865	-1.967128	1.331277	0.005827	0.706125
-30.557179	-2.017871	1.336282	0.005775	0.706125
-30.762609	-1.978125	1.341286	0.005813	0.706131
-31.093358	-1.925434	1.346291	0.005874	0.706118
-30.686755	-1.998166	1.351296	0.005799	0.706118
-31.369392	-2.006801	1.356301	0.005926	0.705856
-31.741567	-1.941017	1.361306	0.005995	0.705855
-31.577895	-1.966758	1.366310	0.005964	0.705862
-31.646631	-1.957977	1.371315	0.005977	0.705855
-31.380782	-2.001738	1.376320	0.005928	0.705862
-31.625682	-1.961282	1.381325	0.005973	0.705856
-31.755331	-2.023129	1.386330	0.005997	0.705685
-32.713821	-1.933203	1.391334	0.006176	0.705522
-32.491031	-1.974528	1.396339	0.006134	0.705519
-32.404593	-1.986736	1.401344	0.006118	0.705525
-32.686059	-1.940767	1.406349	0.006171	0.705517
-32.606640	-1.954594	1.411354	0.006156	0.705518
-32.132762	-2.035986	1.416358	0.006068	0.705524
-32.917096	-2.000004	1.421363	0.006214	0.705315
-34.006042	-1.857386	1.426368	0.006416	0.705211
-33.375394	-1.971188	1.431373	0.006299	0.705209
-33.254165	-1.994679	1.436378	0.006276	0.705205
-33.651324	-1.920367	1.441382	0.006350	0.705212
-33.776363	-1.903251	1.446387	0.006373	0.705202
-33.412211	-1.964736	1.451392	0.006306	0.705208
-33.547942	-1.983590	1.456397	0.006331	0.705122
-34.647238	-1.908637	1.461402	0.006536	0.704878
-34.112084	-1.997860	1.466406	0.006436	0.704891
-34.594460	-1.917811	1.471411	0.006526	0.704879
-34.692641	-1.898349	1.476416	0.006544	0.704883
-34.330866	-1.963794	1.481421	0.006477	0.704881
-34.533358	-1.928836	1.486426	0.006514	0.704879
-34.555002	-1.921353	1.491430	0.006518	0.704886
-34.778772	-2.014062	1.496435	0.006560	0.704619
-35.099157	-1.971449	1.501440	0.006620	0.704590
-35.321851	-1.932850	1.506445	0.006661	0.704587
-35.406442	-1.919763	1.511450	0.006677	0.704583
-35.066633	-1.977186	1.516454	0.006613	0.704590
-35.098736	-1.975354	1.521459	0.006619	0.704582
-35.362309	-1.943373	1.526464	0.006668	0.704552
-35.894304	-1.993569	1.531469	0.006768	0.704260
-35.900730	-1.994494	1.536474	0.006769	0.704255
-36.174229	-1.944474	1.541478	0.006820	0.704258
-36.352734	-1.915842	1.546483	0.006853	0.704252
-35.956024	-1.981206	1.551488	0.006779	0.704262
-35.924470	-1.990218	1.556493	0.006773	0.704256
-36.403310	-1.932354	1.561498	0.006862	0.704200
-36.924904	-1.962888	1.566502	0.006959	0.703951
-36.773642	-1.993783	1.571507	0.006931	0.703943
-37.080996	-1.932580	1.576512	0.006988	0.703956
-36.908811	-1.966277	1.581517	0.006956	0.703950
-36.878931	-1.975182	1.586522	0.006951	0.703943
-37.097387	-1.931841	1.591526	0.006991	0.703952
-37.315067	-1.918628	1.596531	0.007032	0.703900
-37.365890	-2.041975	1.601536	0.007041	0.703633
-37.371301	-2.042691	1.606541	0.007042	0.703630
-38.297594	-1.878488	1.611546	0.007215	0.703628
-37.616445	-1.994495	1.616550	0.007088	0.703639
-37.604053	-2.003028	1.621555	0.007086	0.703626
-38.087875	-1.913033	1.626560	0.007176	0.703634
-38.072914	-1.976556	1.631565	0.007173	0.703511
-38.733755	-1.946488	1.636570	0.007296	0.703334
-38.244211	-2.029421	1.641574	0.007205	0.703343
-39.003529	-1.899894	1.646579	0.007346	0.703331
-38.929215	-1.909412	1.651584	0.007332	0.703339
-38.539502	-1.980422	1.656589	0.007260	0.703336
-38.897188	-1.917943	1.661594	0.007326	0.703333
-38.731128	-2.012168	1.666598	0.007295	0.703203
-39.654204	-1.950411	1.671603	0.007467	0.702995
-39.500651	-1.973363	1.676608	0.007438	0.703004
-39.597526	-1.958621	1.681613	0.007456	0.702999
-39.781597	-1.928215	1.686618	0.007491	0.702994
-39.226714	-2.021758	1.691622	0.007387	0.703005
-39.838307	-1.918333	1.696627	0.007501	0.702994
-39.597832	-2.037308	1.701632	0.007456	0.702840
-40.402129	-1.969711	1.706637	0.007606	0.702687
-40.697015	-1.918155	1.711642	0.007661	0.702685
-40.494746	-1.950684	1.716646	0.007623	0.702692
-40.417958	-1.968643	1.721651	0.007609	0.702683
-40.191161	-2.006628	1.726656	0.007567	0.702688
-40.489040	-1.955387	1.731661	0.007622	0.702685
-40.572859	-2.035775	1.736666	0.007638	0.702492
-41.255082	-1.975463	1.741670	0.007765	0.702368
-41.525455	-1.932676	1.746675	0.007815	0.702357
-41.410257	-1.949683	1.751680	0.007794	0.702364
-41.195626	-1.986929	1.756685	0.007754	0.702366
-41.163536	-1.994445	1.761690	0.007748	0.702363
-41.450441	-1.940334	1.766694	0.007801	0.702369
-41.435294	-2.038052	1.771699	0.007798	0.702177
-42.415815	-1.916878	1.776704	0.007981	0.702068
-42.105110	-1.970253	1.781709	0.007923	0.702072
-42.170188	-1.959516	1.786714	0.007935	0.702071
-42.162563	-1.957421	1.791718	0.007934	0.702078
-42.523814	-1.899816	1.796723	0.008001	0.702064
-42.254863	-1.943546	1.801728	0.007951	0.702073
-42.030358	-2.077975	1.806733	0.007909	0.701882
-43.491978	-1.888615	1.811738	0.008181	0.701738
-43.122902	-1.949739	1.816742	0.008112	0.701747
-42.997392	-1.977190	1.821747	0.008089	0.701737
-43.028948	-1.968033	1.826752	0.008095	0.701744
-43.059665	-1.962805	1.831757	0.008101	0.701744
-43.226680	-1.935588	1.836762	0.008132	0.701738
-43.093993	-2.054215	1.841766	0.008107	0.701546
-44.270207	-1.900825	1.846771	0.008326	0.701432
-44.233384	-1.904055	1.851776	0.008319	0.701439
-43.910207	-1.963629	1.856781	0.008259	0.701435
-44.196359	-1.915821	1.861786	0.008312	0.701429
-44.083821	-1.930857	1.866790	0.008291	0.701439
-44.283744	-1.901162	1.871795	0.008328	0.701427
-44.091552	-1.969801	1.876800	0.008293	0.701357
-44.834373	-1.953949	1.881805	0.008431	0.701121
-44.908371	-1.943816	1.886810	0.008445	0.701115
-44.755299	-1.967739	1.891814	0.008416	0.701122
-44.775726	-1.969201	1.896819	0.008420	0.701112
-44.983060	-1.929049	1.901824	0.008458	0.701118
-44.839093	-1.954585	1.906829	0.008432	0.701118
-44.922396	-1.984062	1.911834	0.008447	0.701029
-45.890884	-1.887463	1.916838	0.008627	0.700874
-45.532312	-1.956585	1.921843	0.008561	0.700864
-45.498344	-1.960041	1.926848	0.008554	0.700869
-45.578255	-1.946464	1.931853	0.008569	0.700868
-45.874654	-1.895784	1.936858	0.008624	0.700864
-45.425860	-1.970980	1.941862	0.008541	0.700873
-45.483280	-2.065636	1.946867	0.008551	0.700661
-46.725568	-1.907076	1.951872	0.008783	0.700533
-46.204692	-1.999866	1.956877	0.008686	0.700534
-46.272861	-1.991385	1.961882	0.008698	0.700526
-46.582063	-1.931913	1.966886	0.008756	0.700535
-46.669917	-1.920615	1.971891	0.008772	0.700526
-46.512715	-1.949283	1.976896	0.008743	0.700525
-47.166410	-1.985887	1.981901	0.008865	0.700214
-47.448054	-1.938719	1.986906	0.008917	0.700208
-47.205861	-1.976117	1.991910	0.008872	0.700220
-47.110350	-1.999018	1.996915	0.008854	0.700208
-47.253656	-1.970863	2.001920	0.008881	0.700213
-47.477004	-1.988901	2.011917	0.008922	0.700096
-48.310659	-1.942460	2.021914	0.009078	0.699889
-48.328097	-1.940619	2.031910	0.009081	0.699886
-47.938323	-2.008626	2.041907	0.009008	0.699889
-48.456857	-1.916188	2.051904	0.009105	0.699889
-48.283257	-1.947530	2.061901	0.009072	0.699889
-48.178902	-1.965985	2.071898	0.009053	0.699889
-48.328143	-1.907592	2.081894	0.009081	0.699954
-47.388979	-1.946479	2.091891	0.008906	0.700215
-47.410631	-1.941845	2.101888	0.008910	0.700216
-47.293656	-1.964630	2.111885	0.008888	0.700212
-47.415670	-1.943139	2.121882	0.008911	0.700212
-47.520605	-1.924500	2.131878	0.008930	0.700212
-47.083733	-2.001521	2.141875	0.008849	0.700214
-47.382857	-1.946749	2.151872	0.008904	0.700217
-46.832898	-1.943620	2.161869	0.008802	0.700422
-46.804109	-1.896559	2.171866	0.008796	0.700528
-46.401519	-1.968851	2.181862	0.008721	0.700527
-46.442865	-1.960204	2.191859	0.008729	0.700530
-46.538726	-1.920245	2.201856	0.008747	0.700576
-45.713771	-1.922942	2.211853	0.008593	0.700869
-45.503430	-1.960526	2.221850	0.008554	0.700869
-45.470516	-1.966354	2.231846	0.008548	0.700869
-45.341437	-1.988599	2.241843	0.008524	0.700870
-45.256323	-1.905907	2.251840	0.008508	0.701069
-44.836508	-1.956730	2.261837	0.008430	0.701118
-44.935397	-1.941525	2.271834	0.008448	0.701113
-44.746382	-1.932474	2.281830	0.008413	0.701199
-43.927138	-1.964354	2.291827	0.008260	0.701431
-43.814861	-1.983871	2.301824	0.008239	0.701432
-43.802959	-1.987419	2.311821	0.008237	0.701429
-43.687109	-1.923023	2.321818	0.008215	0.701601
-43.019325	-1.975638	2.331814	0.008091	0.701736
-43.139662	-1.953676	2.341811	0.008113	0.701737
-42.938300	-1.987378	2.351808	0.008076	0.701741
-42.309010	-1.938963	2.361805	0.007959	0.702066
-42.341784	-1.932421	2.371802	0.007965	0.702068
-42.198985	-1.958809	2.381798	0.007938	0.702066
-41.876912	-1.934890	2.391795	0.007878	0.702231
-41.212007	-1.986383	2.401792	0.007754	0.702366
-41.450952	-1.943930	2.411789	0.007799	0.702366
-41.504163	-1.921605	2.421786	0.007809	0.702392
-40.567416	-1.944211	2.431782	0.007634	0.702684
-40.339563	-1.983675	2.441779	0.007592	0.702687
-40.463594	-1.961403	2.451776	0.007615	0.702687
-40.243997	-1.903545	2.461773	0.007574	0.702883
-39.761324	-1.933852	2.471770	0.007484	0.702996
-39.628287	-1.957105	2.481766	0.007459	0.702997
-39.690836	-1.908803	2.491763	0.007471	0.703072
-38.707329	-1.951632	2.501760	0.007288	0.703340
-38.550663	-1.979562	2.511757	0.007258	0.703340
-38.840981	-1.930314	2.521754	0.007312	0.703335
-38.308823	-1.928127	2.531750	0.007213	0.703531
-38.007297	-1.933050	2.541747	0.007157	0.703629
-37.910263	-1.947908	2.551744	0.007139	0.703634
-37.981818	-1.887043	2.561741	0.007152	0.703731
-37.063287	-1.943220	2.571738	0.006981	0.703948
-37.248724	-1.911164	2.581734	0.007016	0.703947
-37.155486	-1.927281	2.591731	0.006998	0.703948
-36.327539	-1.924825	2.601728	0.006844	0.704250
-36.283205	-1.929393	2.611725	0.006836	0.704257
-36.282467	-1.930452	2.621722	0.006836	0.704255
-35.928959	-1.898990	2.631718	0.006770	0.704446
-35.516217	-1.903815	2.641715	0.006693	0.704584
-35.308141	-1.939124	2.651712	0.006654	0.704588
-35.276864	-1.923908	2.661709	0.006648	0.704630
-34.397515	-1.956184	2.671706	0.006484	0.704881
-34.515751	-1.936111	2.681702	0.006506	0.704879
-34.557325	-1.927107	2.691699	0.006514	0.704882
-34.051915	-1.914133	2.701696	0.006420	0.705090
-33.796706	-1.902878	2.711693	0.006372	0.705204
-33.736979	-1.913329	2.721690	0.006361	0.705205
-33.451657	-1.927932	2.731686	0.006308	0.705278
-32.838529	-1.918098	2.741683	0.006194	0.705518
-32.440682	-1.987931	2.751680	0.006120	0.705520
-32.803136	-1.923082	2.761677	0.006187	0.705520
-32.039329	-1.952418	2.771674	0.006045	0.705735
-31.878646	-1.920603	2.781670	0.006015	0.705857
-31.488492	-1.989373	2.791667	0.005942	0.705859
-31.676079	-1.955115	2.801664	0.005977	0.705860
-31.293108	-1.910714	2.811661	0.005906	0.706087
-31.113501	-1.926052	2.821658	0.005872	0.706121
-31.039879	-1.939174	2.831654	0.005859	0.706121
-30.827982	-1.887486	2.841651	0.005819	0.706301
-30.147393	-1.939273	2.851648	0.005692	0.706441
-30.293811	-1.913754	2.861645	0.005720	0.706439
-30.059841	-1.910497	2.871642	0.005676	0.706530
-29.230869	-1.951475	2.881638	0.005522	0.706744
-29.031108	-1.986107	2.891635	0.005484	0.706746
-29.294055	-1.938028	2.901632	0.005533	0.706749
-28.797592	-1.909539	2.911629	0.005441	0.706984
-28.328572	-1.948414	2.921626	0.005353	0.707074
-28.525393	-1.911966	2.931622	0.005390	0.707077
-28.262232	-1.911026	2.941619	0.005341	0.707173
-27.548145	-1.938311	2.951616	0.005208	0.707374
-27.767956	-1.898972	2.961613	0.005249	0.707374
-27.418080	-1.962424	2.971610	0.005184	0.707372
-27.056445	-1.878039	2.981606	0.005116	0.707671
-26.399062	-1.982780	2.991603	0.004994	0.707696
-26.817387	-1.908487	3.001600	0.005072	0.707695
-26.386596	-1.912711	3.011597	0.004992	0.707841
-25.730855	-1.946566	3.021594	0.004869	0.708007
-25.823951	-1.930204	3.031590	0.004887	0.708007
-25.528470	-1.980489	3.041587	0.004832	0.708012
-25.130184	-1.909707	3.051584	0.004757	0.708296
-24.759275	-1.950424	3.061581	0.004688	0.708347
-24.760133	-1.950775	3.071578	0.004688	0.708346
-24.838958	-1.906613	3.081574	0.004703	0.708406
-23.875831	-1.964201	3.091571	0.004524	0.708635
-23.965277	-1.947710	3.101568	0.004540	0.708636
-24.109912	-1.922943	3.111565	0.004567	0.708634
-23.612533	-1.881946	3.121562	0.004475	0.708894
-23.420367	-1.887931	3.131558	0.004439	0.708950
-23.105466	-1.944521	3.141555	0.004380	0.708950
-23.051134	-1.873309	3.151552	0.004370	0.709112
-22.220487	-1.945942	3.161549	0.004215	0.709263
-22.379654	-1.917689	3.171546	0.004245	0.709262
-22.112824	-1.966218	3.181542	0.004195	0.709261
-21.491784	-1.910368	3.191539	0.004079	0.709594
-21.372631	-1.931640	3.201536	0.004057	0.709594
-21.323107	-1.940620	3.211533	0.004048	0.709594
-21.337550	-1.868095	3.221530	0.004051	0.709734
-20.559380	-1.929345	3.231526	0.003906	0.709888
-20.581821	-1.924131	3.241523	0.003910	0.709891
-20.473880	-1.936524	3.251520	0.003890	0.709905
-19.727792	-1.914491	3.261517	0.003751	0.710215
-19.775699	-1.906811	3.271514	0.003760	0.710213
-19.687345	-1.921654	3.281510	0.003743	0.710215
-19.409512	-1.876312	3.291507	0.003691	0.710404
-18.629242	-1.950335	3.301504	0.003546	0.710534
-18.784563	-1.923709	3.311501	0.003575	0.710532
-18.887702	-1.895271	3.321498	0.003594	0.710552
-18.098909	-1.878658	3.331494	0.003447	0.710866
-17.702365	-1.948224	3.341491	0.003373	0.710869
-17.971778	-1.898332	3.351488	0.003423	0.710872
-17.483075	-1.908641	3.361485	0.003332	0.711026
-17.255401	-1.893369	3.371482	0.003290	0.711137
-17.098915	-1.922466	3.381478	0.003261	0.711135
-17.183354	-1.877221	3.391475	0.003276	0.711195
-16.383796	-1.890034	3.401472	0.003127	0.711454
-16.310937	-1.902897	3.411469	0.003114	0.711454
-16.494458	-1.871524	3.421466	0.003148	0.711452
-15.589290	-1.889150	3.431462	0.002979	0.711738
-15.349993	-1.920852	3.441459	0.002935	0.711760
-15.542293	-1.886152	3.451456	0.002971	0.711761
-14.986718	-1.900547	3.461453	0.002867	0.711930
-14.381576	-1.930732	3.471450	0.002754	0.712085
-14.270581	-1.949174	3.481446	0.002734	0.712087
-14.284792	-1.945697	3.491443	0.002736	0.712089
-13.591653	-1.979774	3.501440	0.002607	0.712268
-13.239839	-1.982984	3.511437	0.002542	0.712386
-13.523432	-1.932882	3.521434	0.002594	0.712385
-13.151971	-2.000479	3.531430	0.002525	0.712383
-12.775961	-1.945512	3.541427	0.002455	0.712626
-12.339903	-1.981011	3.551424	0.002374	0.712710
-12.365622	-1.976896	3.561421	0.002379	0.712709
-12.543967	-1.940445	3.571418	0.002412	0.712718
-11.634081	-1.950028	3.581414	0.002242	0.713022
-11.716197	-1.934059	3.591411	0.002258	0.713025
-11.288295	-2.010455	3.601408	0.002178	0.713024
-11.465803	-1.902355	3.611405	0.002211	0.713177
-10.506422	-1.981987	3.621402	0.002032	0.713358
-10.696141	-1.947082	3.631398	0.002068	0.713361
-10.428477	-1.993708	3.641395	0.002018	0.713363
-10.011663	-1.976486	3.651392	0.001940	0.713545
-9.604558	-1.995759	3.661389	0.001864	0.713651
-9.807418	-1.960988	3.671386	0.001902	0.713648
-9.608922	-1.995093	3.681382	0.001865	0.713651
-8.960495	-1.959289	3.691379	0.001744	0.713952
-8.474231	-2.036836	3.701376	0.001654	0.713970
-8.726799	-1.992267	3.711373	0.001701	0.713969
-8.946179	-1.923722	3.721370	0.001741	0.714028
-8.018276	-1.964968	3.731366	0.001569	0.714274
-7.954192	-1.975399	3.741363	0.001557	0.714276
-8.008073	-1.965521	3.751360	0.001567	0.714277
-7.455728	-1.922689	3.761357	0.001464	0.714557
-7.007508	-1.980063	3.771354	0.001380	0.714602
-6.921301	-1.995025	3.781350	0.001364	0.714603
-6.826973	-1.982225	3.791347	0.001347	0.714662
-5.947141	-2.014350	3.801344	0.001183	0.714909
-6.103432	-1.988197	3.811341	0.001212	0.714906
-6.001171	-2.006845	3.821338	0.001193	0.714905
-5.789348	-1.959507	3.831334	0.001153	0.715074
-5.019216	-2.018818	3.841331	0.001010	0.715229
-5.181317	-1.989031	3.851328	0.001040	0.715231
-5.460083	-1.940076	3.861325	0.001092	0.715229
-4.516132	-1.951312	3.871322	0.000916	0.715540
-4.265527	-1.994100	3.881318	0.000869	0.715544
-4.106527	-2.022540	3.891315	0.000840	0.715544
-4.034134	-1.977603	3.901312	0.000826	0.715659
-3.176390	-2.016958	3.911309	0.000666	0.715884
-3.181756	-2.017537	3.921306	0.000667	0.715881
-3.279892	-2.001078	3.931302	0.000686	0.715879
-3.034477	-1.991391	3.941299	0.000640	0.715985
-2.447179	-2.021887	3.951296	0.000530	0.716132
-2.631787	-1.988328	3.961293	0.000565	0.716133
-2.556123	-1.994189	3.971290	0.000551	0.716148
-1.798538	-1.979779	3.981286	0.000410	0.716444
-1.818128	-1.976918	3.991283	0.000413	0.716443
-1.801246	-1.979330	4.001280	0.000410	0.716444
-1.571994	-1.903790	4.011277	0.000367	0.716675
-1.370890	-1.900362	4.021274	0.000330	0.716752
-1.409299	-1.894228	4.031270	0.000337	0.716751
-1.265502	-1.767271	4.041267	0.000310	0.717053
-1.166564	-1.769089	4.051264	0.000291	0.717084
-1.114804	-1.709798	4.061261	0.000282	0.717220
-1.050219	-1.643490	4.071258	0.000270	0.717374
-1.074359	-1.589467	4.081254	0.000274	0.717472
-1.131675	-1.464531	4.091251	0.000285	0.717699
-0.911044	-1.436208	4.101248	0.000244	0.717833
-0.966615	-1.334073	4.111245	0.000254	0.718015
-0.848061	-1.240850	4.121242	0.000232	0.718241
-0.704114	-1.207522	4.131238	0.000205	0.718358
-0.646794	-1.074674	4.141235	0.000194	0.718640
-0.567443	-1.012424	4.151232	0.000179	0.718791
-0.559970	-0.927455	4.161229	0.000178	0.718961
-0.574225	-0.770009	4.171226	0.000180	0.719267
-0.621102	-0.655683	4.181222	0.000189	0.719476
-0.452692	-0.572927	4.191219	0.000157	0.719698
-0.383564	-0.473366	4.201216	0.000144	0.719919
-0.475075	-0.304177	4.211213	0.000161	0.720220
-0.347365	-0.186349	4.221210	0.000137	0.720497
-0.210426	-0.067648	4.231206	0.000112	0.720779
-0.152027	0.042454	4.241203	0.000101	0.721016
0.000000	0.175383	4.251200	0.000072	0.721331
0.012908	0.818382	4.256205	0.000069	0.722599
0.057150	2.077670	4.261210	0.000060	0.725082
0.373199	3.876296	4.266214	0.000000	0.728702
0.448057	6.268524	4.271219	-0.000015	0.733370
0.606508	9.156636	4.276224	-0.000047	0.738989
1.058974	12.467508	4.281229	-0.000133	0.745470
1.452587	16.253082	4.286234	-0.000209	0.752771
1.835637	20.440737	4.291238	-0.000283	0.760748
2.175100	25.031580	4.296243	-0.000349	0.769371
2.691443	29.969508	4.301248	-0.000449	0.778588
3.192378	35.248332	4.306253	-0.000545	0.788306
3.578996	40.870862	4.311258	-0.000621	0.798481
4.057438	46.781598	4.316262	-0.000714	0.809061
4.594572	52.958887	4.321267	-0.000818	0.819983
4.976063	59.445284	4.326272	-0.000893	0.831242
5.406142	66.137854	4.331277	-0.000978	0.842712
5.845884	73.053963	4.336282	-0.001064	0.854401
9.469570	79.638722	4.341286	-0.001743	0.866308
9.908978	87.002250	4.346291	-0.001830	0.878405
10.831511	94.458616	4.351296	-0.002006	0.890620
12.358328	101.966084	4.356301	-0.002296	0.902916
12.815696	109.818640	4.361306	-0.002386	0.915290
14.071744	117.647409	4.366310	-0.002625	0.927676
15.192530	125.625151	4.371315	-0.002839	0.940088
16.313685	133.727438	4.376320	-0.003053	0.952522
17.296807	141.936823	4.381325	-0.003241	0.964917
17.844811	150.296481	4.386330	-0.003349	0.977263
18.673277	158.705323	4.391334	-0.003509	0.989595
19.359683	167.159846	4.396339	-0.003642	1.001804
20.631901	175.553203	4.401344	-0.003884	1.013922
21.557403	184.046807	4.406349	-0.004062	1.025952
22.147172	192.642000	4.411354	-0.004178	1.037901
22.880440	201.238768	4.416358	-0.004320	1.049750
23.553463	209.861260	4.421363	-0.004451	1.061486
25.376891	218.334959	4.426368	-0.004796	1.073160
26.211227	226.976149	4.431373	-0.004957	1.084702
26.813217	235.667768	4.436378	-0.005075	1.096137
27.490088	244.347287	4.441382	-0.005206	1.107453
28.307278	252.997863	4.446387	-0.005364	1.118649
29.104575	261.658960	4.451392	-0.005518	1.129742
30.385092	270.236506	4.456397	-0.005762	1.140727
30.720641	278.996593	4.461402	-0.005830	1.151631
31.396489	287.662634	4.466406	-0.005962	1.162389
31.903088	296.324099	4.471411	-0.006062	1.173007
32.353402	304.986241	4.476416	-0.006151	1.183520
33.251086	313.559858	4.481421	-0.006324	1.193925
34.178957	322.101922	4.486426	-0.006503	1.204208
34.869486	330.702227	4.491430	-0.006637	1.214425
35.718792	339.243249	4.496435	-0.006800	1.224519
36.693033	347.799381	4.501440	-0.006987	1.234571
37.464447	356.332315	4.506445	-0.007137	1.244477
37.981790	364.905111	4.511450	-0.007239	1.254300
38.740772	373.420266	4.516454	-0.007386	1.264028
39.501430	381.921849	4.521459	-0.007533	1.273666
40.315898	390.401935	4.526464	-0.007690	1.283218
40.615042	398.959860	4.531469	-0.007751	1.292689
41.449601	407.406384	4.536474	-0.007912	1.302068
42.878897	415.843022	4.541478	-0.008184	1.311476
43.464410	424.353624	4.546483	-0.008298	1.320745
44.283875	432.766517	4.551488	-0.008456	1.329886
45.298846	441.144521	4.556493	-0.008651	1.338962
45.780362	449.589566	4.561498	-0.008746	1.347954
45.889232	458.097396	4.566502	-0.008772	1.356886
46.430016	466.472854	4.571507	-0.008878	1.365697
47.286645	474.830175	4.576512	-0.009043	1.374487
48.060602	483.174295	4.581517	-0.009193	1.383193
48.715838	491.554226	4.586522	-0.009320	1.391860
49.342747	499.916089	4.591526	-0.009442	1.400451
49.937973	508.261037	4.596531	-0.009559	1.408967
50.379748	516.640798	4.601536	-0.009646	1.417440
50.943996	524.973116	4.606541	-0.009757	1.425837
51.588394	533.312185	4.611546	-0.009882	1.434203
52.295066	541.605318	4.616550	-0.010019	1.442486
52.956576	549.904734	4.621555	-0.010148	1.450720
53.574948	558.218870	4.626560	-0.010269	1.458914
54.094986	566.532799	4.631565	-0.010371	1.467047
54.993509	574.837752	4.636570	-0.010544	1.475186
55.513297	583.135006	4.641574	-0.010646	1.483213
55.870350	591.437215	4.646579	-0.010718	1.491176
56.336940	599.739687	4.651584	-0.010810	1.499114
56.867316	608.004852	4.656589	-0.010914	1.506985
56.912193	616.357547	4.661594	-0.010928	1.514822
57.404261	624.613216	4.666598	-0.011025	1.522596
57.679207	632.883989	4.671603	-0.011082	1.530312
58.504005	641.091529	4.676608	-0.011240	1.538014
59.366913	649.271735	4.681613	-0.011407	1.545657
59.969965	657.534608	4.686618	-0.011524	1.553299
60.674262	665.744660	4.691622	-0.011661	1.560870
60.946779	674.014254	4.696627	-0.011717	1.568396
61.196701	682.297379	4.701632	-0.011769	1.575894
61.888915	690.486375	4.706637	-0.011903	1.583336
62.734801	698.667413	4.711642	-0.012066	1.590758
63.013295	706.948095	4.716646	-0.012123	1.598153
63.198228	715.182904	4.721651	-0.012163	1.605460
64.042252	723.364373	4.726656	-0.012326	1.612780
64.566131	731.579053	4.731661	-0.012428	1.620050
64.871859	739.815596	4.736666	-0.012491	1.627277
65.334099	748.099637	4.741670	-0.012582	1.634534
65.798827	756.256712	4.746675	-0.012674	1.641650
66.046945	764.480082	4.751680	-0.012726	1.648762
66.560963	772.667753	4.756685	-0.012827	1.655849
67.193138	780.811650	4.761690	-0.012950	1.662885
67.672859	789.013501	4.766694	-0.013044	1.669919
68.027079	797.220119	4.771699	-0.013116	1.676911
68.508327	805.389875	4.776704	-0.013211	1.683860
68.945134	813.575053	4.781709	-0.013297	1.690787
69.025394	821.814884	4.786714	-0.013318	1.697684
69.978966	829.926319	4.791718	-0.013501	1.704561
70.314814	838.134928	4.796723	-0.013569	1.711410
70.591183	846.346391	4.801728	-0.013625	1.718226
71.010918	854.491611	4.806733	-0.013709	1.724979
71.276774	862.675047	4.811738	-0.013764	1.731717
71.766081	870.841833	4.816742	-0.013860	1.738444
72.218800	878.972055	4.821747	-0.013950	1.745111
72.866474	887.117081	4.826752	-0.014076	1.751789
73.455196	895.263722	4.831757	-0.014191	1.758434
73.636877	903.434075	4.836762	-0.014230	1.765023
73.948171	911.633342	4.841766	-0.014293	1.771627
74.201476	919.804143	4.846771	-0.014346	1.778176
74.478462	927.962904	4.851776	-0.014403	1.784694
75.128081	936.106011	4.856781	-0.014529	1.791222
75.378705	944.298120	4.861786	-0.014581	1.797716
75.788556	952.439776	4.866790	-0.014663	1.804166
76.214867	960.547357	4.871795	-0.014747	1.810568
76.805133	968.675985	4.876800	-0.014862	1.816984
77.403614	976.787026	4.881805	-0.014979	1.823364
77.778834	984.931395	4.886810	-0.015054	1.829721
78.077868	993.106268	4.891814	-0.015115	1.836070
78.564147	1001.215568	4.896819	-0.015211	1.842370
78.998869	1009.352856	4.901824	-0.015297	1.848662
79.550147	1017.486534	4.906829	-0.015405	1.854945
79.807130	1025.634041	4.911834	-0.015459	1.861182
80.301323	1033.774744	4.916838	-0.015556	1.867420
80.762462	1041.930012	4.921843	-0.015647	1.873645
81.469730	1050.007749	4.926848	-0.015784	1.879819
82.270628	1058.088469	4.931853	-0.015939	1.885985
82.331763	1066.275670	4.936858	-0.015955	1.892127
82.827917	1074.417643	4.941862	-0.016053	1.898264
83.204894	1082.525957	4.946867	-0.016129	1.904343
83.429865	1090.695146	4.951872	-0.016176	1.910431
83.704275	1098.846785	4.956877	-0.016232	1.916491
84.083273	1106.944663	4.961882	-0.016308	1.922505
84.460209	1115.066648	4.966886	-0.016384	1.928517
84.609816	1123.222334	4.971891	-0.016417	1.934510
85.157014	1131.297632	4.976896	-0.016524	1.940469
86.040502	1139.359527	4.981901	-0.016694	1.946437
86.101190	1147.564385	4.986906	-0.016710	1.952400
86.498784	1155.687974	4.991910	-0.016790	1.958323
87.121408	1163.725716	4.996915	-0.016911	1.964191
88.087500	1171.768864	5.001920	-0.017096	1.970081
88.673873	1179.897961	5.006925	-0.017211	1.975975
89.392397	1187.957823	5.011930	-0.017350	1.981816
89.908217	1196.083663	5.016934	-0.017451	1.987664
89.897965	1204.277579	5.021939	-0.017454	1.993489
90.223960	1212.397030	5.026944	-0.017520	1.999279
90.746819	1220.469098	5.031949	-0.017623	2.005039
91.314854	1228.564350	5.036954	-0.017734	2.010803
91.665550	1236.713238	5.041958	-0.017805	2.016567
92.035833	1244.802989	5.046963	-0.017879	2.022274
92.383192	1252.930258	5.051968	-0.017949	2.027989
92.768123	1261.079035	5.056973	-0.018026	2.033706
93.199607	1269.149515	5.061978	-0.018112	2.039358
93.726242	1277.229900	5.066982	-0.018215	2.045010
93.961402	1285.352994	5.071987	-0.018264	2.050647
94.428854	1293.461667	5.076992	-0.018356	2.056282
94.931144	1301.542156	5.081997	-0.018455	2.061885
95.145579	1309.643309	5.087002	-0.018500	2.067459
95.705006	1317.755738	5.092006	-0.018610	2.073059
96.493419	1325.788174	5.097011	-0.018762	2.078612
97.303584	1333.823927	5.102016	-0.018918	2.084155
97.835026	1341.915543	5.107021	-0.019022	2.089694
98.123616	1350.063376	5.112026	-0.019081	2.095231
98.719106	1358.153302	5.117030	-0.019198	2.100745
98.886562	1366.278575	5.122035	-0.019234	2.106227
99.059265	1374.455857	5.127040	-0.019272	2.111729
99.593885	1382.547021	5.132045	-0.019376	2.117195
99.981101	1390.600670	5.137050	-0.019454	2.122607
100.141191	1398.721496	5.142054	-0.019489	2.128028
100.386530	1406.814430	5.147059	-0.019540	2.133425
100.654372	1414.907601	5.152064	-0.019595	2.138811
101.094697	1422.976556	5.157069	-0.019682	2.144183
101.458871	1431.050907	5.162074	-0.019755	2.149538
102.101620	1439.137721	5.167078	-0.019880	2.154914
102.329705	1447.218138	5.172083	-0.019928	2.160234
102.394988	1455.333982	5.177088	-0.019946	2.165548
103.133444	1463.363451	5.182093	-0.020088	2.170856
103.425191	1471.464395	5.187098	-0.020148	2.176155
103.764470	1479.551852	5.192102	-0.020216	2.181438
104.345551	1487.596663	5.197107	-0.020330	2.186702
104.844120	1495.703704	5.202112	-0.020428	2.191985
105.205323	1503.807193	5.207117	-0.020501	2.197242
105.671586	1511.839946	5.212122	-0.020593	2.202449
106.335683	1519.898035	5.217126	-0.020722	2.207679
106.571992	1528.023993	5.222131	-0.020771	2.212900
106.724114	1536.138575	5.227136	-0.020804	2.218095
107.156460	1544.189042	5.232141	-0.020890	2.223262
107.545915	1552.272937	5.237146	-0.020968	2.228433
107.834610	1560.398149	5.242150	-0.021027	2.233611
107.877252	1568.493077	5.247155	-0.021040	2.238735
108.516977	1576.506396	5.252160	-0.021165	2.243848
108.716440	1584.624416	5.257165	-0.021207	2.248977
108.765807	1592.740227	5.262170	-0.021222	2.254080
109.326591	1600.781437	5.267174	-0.021331	2.259169
109.614197	1608.839880	5.272179	-0.021390	2.264233
109.961660	1616.918802	5.277184	-0.021460	2.269305
110.724884	1625.046355	5.282189	-0.021608	2.274430
111.250884	1633.042436	5.287194	-0.021711	2.279442
111.809820	1641.083717	5.292198	-0.021820	2.284474
112.403471	1649.128237	5.297203	-0.021936	2.289500
112.818631	1657.225812	5.302208	-0.022018	2.294531
112.988245	1665.320137	5.307213	-0.022055	2.299529
113.288935	1673.388522	5.312218	-0.022117	2.304512
113.798310	1681.467653	5.317222	-0.022217	2.309507
114.283730	1689.528577	5.322227	-0.022312	2.314479
114.357703	1697.627824	5.327232	-0.022331	2.319428
114.673530	1705.699627	5.332237	-0.022396	2.324371
115.147700	1713.737951	5.337242	-0.022489	2.329296
115.493280	1721.853377	5.342246	-0.022559	2.334246
115.699994	1729.916842	5.347251	-0.022603	2.339143
116.237178	1737.949152	5.352256	-0.022708	2.344038
116.496635	1746.048444	5.357261	-0.022761	2.348941
116.711619	1754.151633	5.362266	-0.022807	2.353831
116.873282	1762.234772	5.367270	-0.022842	2.358696
117.204224	1770.265963	5.372275	-0.022909	2.363532
117.425149	1778.344866	5.377280	-0.022955	2.368379
117.830852	1786.412217	5.382285	-0.023036	2.373223
118.139593	1794.468931	5.387290	-0.023099	2.378044
118.378006	1802.529018	5.392294	-0.023149	2.382851
118.515677	1810.621678	5.397299	-0.023180	2.387659
119.256543	1818.660393	5.402304	-0.023323	2.392474
119.739769	1826.712360	5.407309	-0.023418	2.397266
120.182393	1834.743755	5.412314	-0.023506	2.402033
120.971277	1842.783836	5.417318	-0.023658	2.406823
121.202878	1850.873815	5.422323	-0.023706	2.411589
121.435467	1858.966224	5.427328	-0.023755	2.416347
121.793032	1867.021830	5.432333	-0.023827	2.421084
122.036449	1875.085532	5.437338	-0.023877	2.425808
122.348136	1883.195008	5.442342	-0.023941	2.430554
122.363592	1891.347539	5.447347	-0.023949	2.435293
122.837882	1899.336445	5.452352	-0.024042	2.439963
123.401571	1907.329750	5.457357	-0.024153	2.444633
123.599532	1915.394062	5.462362	-0.024195	2.449308
123.895258	1923.478975	5.467366	-0.024255	2.453993
124.184914	1931.532014	5.472371	-0.024314	2.458650
124.567778	1939.571465	5.477376	-0.024391	2.463297
125.047645	1947.621043	5.482381	-0.024485	2.467949
125.119025	1955.716184	5.487386	-0.024504	2.472587
125.448974	1963.780334	5.492390	-0.024571	2.477218
125.870235	1971.815041	5.497395	-0.024654	2.481831
126.279000	1979.857260	5.502400	-0.024736	2.486438
126.438122	1987.951421	5.507405	-0.024771	2.491047
126.587508	1996.024193	5.512410	-0.024804	2.495636
127.014682	2004.076031	5.517414	-0.024889	2.500224
127.173941	2012.116104	5.522419	-0.024924	2.504778
127.248779	2020.188999	5.527424	-0.024943	2.509335
127.831822	2028.259278	5.532429	-0.025057	2.513920
128.224325	2036.276811	5.537434	-0.025135	2.518453
128.730997	2044.302759	5.542438	-0.025235	2.522990
128.997394	2052.354151	5.547443	-0.025289	2.527516
129.165722	2060.456734	5.552448	-0.025326	2.532056
129.899034	2068.479445	5.557453	-0.025468	2.536583
130.283424	2076.517088	5.562458	-0.025545	2.541086
130.556792	2084.590110	5.567462	-0.025601	2.545592
130.809662	2092.651496	5.572467	-0.025653	2.550083
131.250489	2100.713567	5.577472	-0.025741	2.554579
131.661959	2108.765015	5.582477	-0.025822	2.559059
131.775787	2116.813557	5.587482	-0.025849	2.563509
132.349410	2124.857803	5.592486	-0.025961	2.567980
132.626590	2132.927388	5.597491	-0.026018	2.572437
133.083027	2140.979474	5.602496	-0.026108	2.576889
133.771595	2149.012606	5.607501	-0.026242	2.581339
133.918312	2157.054350	5.612506	-0.026274	2.585749
134.424999	2165.121170	5.617510	-0.026374	2.590189
134.694211	2173.382303	5.622515	-0.026429	2.594712
135.052826	2181.355208	5.627520	-0.026501	2.599076
135.185373	2189.384879	5.632525	-0.026531	2.603448
135.226590	2197.422804	5.637530	-0.026544	2.607810
135.656236	2205.468343	5.642534	-0.026629	2.612196
136.072289	2213.494101	5.647539	-0.026712	2.616563
136.284256	2221.523789	5.652544	-0.026757	2.620911
136.786422	2229.531040	5.657549	-0.026856	2.625259
136.794952	2237.615179	5.662554	-0.026862	2.629608
137.056201	2245.703945	5.667558	-0.026916	2.633969
137.515255	2253.704411	5.672563	-0.027007	2.638288
137.837311	2261.729567	5.677568	-0.027072	2.642605
138.183246	2269.788502	5.682573	-0.027142	2.646934
138.465058	2277.832976	5.687578	-0.027200	2.651244
138.918965	2285.908083	5.692582	-0.027290	2.655575
139.220178	2293.933627	5.697587	-0.027351	2.659862
139.487329	2301.982934	5.702592	-0.027406	2.664153
140.083804	2310.025321	5.707597	-0.027522	2.668454
140.103122	2318.129959	5.712602	-0.027531	2.672744
140.466928	2326.172704	5.717606	-0.027604	2.677016
140.914289	2334.168043	5.722611	-0.027693	2.681262
141.165489	2342.212518	5.727616	-0.027745	2.685515
141.500266	2350.263368	5.732621	-0.027812	2.689769
141.698707	2358.336469	5.737626	-0.027855	2.694019
142.362936	2366.347284	5.742630	-0.027983	2.698260
142.552801	2374.400654	5.747635	-0.028024	2.702486
142.633130	2382.472718	5.752640	-0.028044	2.706709
143.183440	2390.531077	5.757645	-0.028152	2.710947
143.361174	2398.592354	5.762650	-0.028190	2.715157
143.761708	2406.609602	5.767654	-0.028270	2.719351
144.116456	2414.628077	5.772659	-0.028342	2.723536
144.426865	2422.687278	5.777664	-0.028405	2.727733
144.743444	2430.768606	5.782669	-0.028469	2.731936
144.856503	2438.834726	5.787674	-0.028495	2.736112
145.254130	2446.870451	5.792678	-0.028574	2.740283
145.384224	2454.908451	5.797683	-0.028604	2.744432
145.580206	2462.961851	5.802688	-0.028646	2.748587
145.903709	2471.082475	5.807693	-0.028711	2.752778
146.101044	2479.119645	5.812698	-0.028753	2.756912
146.451359	2487.128456	5.817702	-0.028824	2.761035
146.792832	2495.115043	5.822707	-0.028892	2.765139
147.069099	2503.145807	5.827712	-0.028949	2.769256
147.281740	2511.252503	5.832717	-0.028994	2.773402
147.247818	2519.294667	5.837722	-0.028993	2.777494
147.800925	2527.298732	5.842726	-0.029101	2.781595
148.095406	2535.324079	5.847731	-0.029161	2.785686
148.324239	2543.359155	5.852736	-0.029209	2.789772
148.824642	2551.424676	5.857741	-0.029308	2.793883
149.146135	2559.442074	5.862746	-0.029373	2.797953
149.626433	2567.465991	5.867750	-0.029467	2.802030
149.650024	2575.535937	5.872755	-0.029477	2.806097
150.014024	2583.572213	5.877760	-0.029550	2.810161
150.200493	2591.671210	5.882765	-0.029590	2.814241
150.225869	2599.699039	5.887770	-0.029600	2.818270
150.833080	2607.697926	5.892774	-0.029718	2.822311
150.928008	2615.764704	5.897779	-0.029741	2.826352
151.245475	2623.798293	5.902784	-0.029806	2.830383
151.604492	2631.903301	5.907789	-0.029878	2.834446
151.924030	2639.872834	5.912794	-0.029943	2.838433
152.033936	2647.934098	5.917798	-0.029968	2.842449
152.263589	2655.978157	5.922803	-0.030016	2.846457
152.576031	2664.006680	5.927808	-0.030080	2.850456
152.871235	2672.068792	5.932813	-0.030140	2.854465
153.009844	2680.091845	5.937818	-0.030171	2.858441
153.464648	2688.105100	5.942822	-0.030261	2.862423
153.722974	2696.164525	5.947827	-0.030314	2.866412
153.902128	2704.205512	5.952832	-0.030353	2.870382
154.218450	2712.281760	5.957837	-0.030417	2.874372
154.619165	2720.281091	5.962842	-0.030497	2.878322
154.745897	2728.329225	5.967846	-0.030526	2.882276
154.924220	2736.382738	5.972851	-0.030564	2.886230
155.345226	2744.382083	5.977856	-0.030648	2.890166
155.656207	2752.464908	5.982861	-0.030711	2.894130
155.934222	2760.490268	5.987866	-0.030768	2.898060
156.391536	2768.508764	5.992870	-0.030859	2.901990
156.594714	2776.572234	5.997875	-0.030902	2.905923
156.754445	2784.623237	6.002880	-0.030937	2.909842
157.065510	2792.768358	6.007885	-0.031000	2.913810
157.567808	2800.730272	6.012890	-0.031099	2.917694
157.775184	2808.765763	6.017894	-0.031143	2.921592
157.834449	2816.804392	6.022899	-0.031159	2.925479
158.144538	2824.797855	6.027904	-0.031222	2.929352
158.334852	2832.876080	6.032909	-0.031263	2.933255
158.581925	2840.894720	6.037914	-0.031314	2.937126
158.971982	2848.915040	6.042918	-0.031392	2.941001
159.085273	2856.952095	6.047923	-0.031418	2.944864
159.233705	2864.982929	6.052928	-0.031451	2.948721
159.730239	2873.023936	6.057933	-0.031549	2.952596
160.358356	2881.034134	6.062938	-0.031671	2.956458
160.652903	2889.062935	6.067942	-0.031731	2.960306
160.748551	2897.118488	6.072947	-0.031754	2.964151
160.985688	2905.146415	6.077952	-0.031803	2.967986
161.500107	2913.204425	6.082957	-0.031904	2.971844
161.608594	2921.263310	6.087962	-0.031930	2.975677
162.031455	2929.271435	6.092966	-0.032014	2.979497
162.530661	2937.297102	6.097971	-0.032112	2.983324
162.713380	2945.341246	6.102976	-0.032151	2.987139
162.959162	2953.414208	6.107981	-0.032202	2.990965
163.228163	2961.470029	6.112986	-0.032258	2.994780
163.502816	2969.475349	6.117990	-0.032314	2.998566
163.819599	2977.502422	6.122995	-0.032378	3.002360
163.924870	2985.548150	6.128000	-0.032403	3.006148
164.245261	2993.562167	6.133005	-0.032468	3.009926
164.291808	3001.630497	6.138010	-0.032482	3.013711
164.729309	3009.654699	6.143014	-0.032569	3.017490
164.856271	3017.700966	6.148019	-0.032598	3.021260
165.105494	3025.685074	6.153024	-0.032649	3.025002
165.183727	3033.787415	6.158029	-0.032669	3.028786
165.431572	3041.824639	6.163034	-0.032721	3.032543
165.989447	3049.832403	6.168038	-0.032830	3.036296
166.273536	3057.829001	6.173043	-0.032888	3.040027
166.421676	3065.868476	6.178048	-0.032921	3.043766
166.677738	3073.938450	6.183053	-0.032974	3.047520
166.733857	3081.989191	6.188058	-0.032989	3.051251
167.001983	3090.017891	6.193062	-0.033045	3.054977
167.156801	3098.069520	6.198067	-0.033079	3.058703
167.112339	3106.095272	6.203072	-0.033076	3.062404
167.428041	3114.146769	6.208077	-0.033140	3.066129
167.681204	3122.154203	6.213082	-0.033192	3.069827
168.276349	3130.247365	6.218086	-0.033308	3.073575
168.704687	3138.273784	6.223091	-0.033393	3.077280
168.896127	3146.273510	6.228096	-0.033434	3.080958
169.430373	3154.250914	6.233101	-0.033539	3.084636
169.683423	3162.294538	6.238106	-0.033591	3.088328
169.822958	3170.355954	6.243110	-0.033622	3.092018
170.163704	3178.404084	6.248115	-0.033691	3.095706
170.585655	3186.391470	6.253120	-0.033775	3.099367
170.853201	3194.458896	6.258125	-0.033830	3.103052
171.187604	3202.459296	6.263130	-0.033897	3.106705
171.747004	3210.465383	6.268134	-0.034007	3.110367
171.958277	3218.555154	6.273139	-0.034051	3.114047
172.110097	3226.579864	6.278144	-0.034085	3.117690
172.544838	3234.621839	6.283149	-0.034171	3.121349
172.695978	3242.586188	6.288154	-0.034205	3.124956
172.791328	3250.674647	6.293158	-0.034228	3.128613
173.142930	3258.727241	6.298163	-0.034298	3.132260
173.224239	3266.781365	6.303168	-0.034319	3.135892
173.485921	3274.784094	6.308173	-0.034373	3.139504
173.536884	3282.791837	6.313178	-0.034387	3.143106
173.953722	3290.832805	6.318182	-0.034470	3.146734
174.136463	3298.881769	6.323187	-0.034510	3.150351
174.301735	3306.959224	6.328192	-0.034546	3.153976
174.789448	3314.967887	6.333197	-0.034642	3.157580
174.936851	3322.970780	6.338202	-0.034674	3.161162
175.104916	3330.968931	6.343206	-0.034711	3.164739
175.529088	3339.010294	6.348211	-0.034795	3.168343
175.848132	3347.031201	6.353216	-0.034860	3.171928
176.174876	3355.097828	6.358221	-0.034926	3.175531
176.237510	3363.102166	6.363226	-0.034943	3.179090
176.736716	3371.127801	6.368230	-0.035041	3.182673
177.176264	3379.166339	6.373235	-0.035128	3.186255
177.135396	3387.217044	6.378240	-0.035126	3.189818
177.547519	3395.265301	6.383245	-0.035208	3.193395
177.869431	3403.282599	6.388250	-0.035273	3.196951
178.336423	3411.294496	6.393254	-0.035365	3.200506
178.329260	3419.341366	6.398259	-0.035369	3.204053
178.785463	3427.344090	6.403264	-0.035459	3.207596
179.156407	3435.413659	6.408269	-0.035534	3.211161
179.356266	3443.444518	6.413274	-0.035576	3.214697
179.514647	3451.484668	6.418278	-0.035611	3.218232
179.855272	3459.518780	6.423283	-0.035680	3.221768
179.913307	3467.523441	6.428288	-0.035696	3.225276
180.284747	3475.563266	6.433293	-0.035770	3.228808
180.458399	3483.630529	6.438298	-0.035808	3.232340
180.718965	3491.712219	6.443302	-0.035861	3.235878
181.015933	3499.666958	6.448307	-0.035922	3.239358
181.138994	3507.685968	6.453312	-0.035950	3.242855
181.456806	3515.722260	6.458317	-0.036014	3.246364
181.498328	3523.721743	6.463322	-0.036027	3.249842
181.927697	3531.779019	6.468326	-0.036113	3.253357
182.325163	3539.834470	6.473331	-0.036192	3.256865
182.259932	3547.854699	6.478336	-0.036185	3.260337
182.777823	3555.864025	6.483341	-0.036287	3.263823
182.976441	3563.886753	6.488346	-0.036329	3.267298
183.026776	3571.928019	6.493350	-0.036344	3.270772
183.473697	3579.974402	6.498355	-0.036432	3.274260
183.733712	3587.951567	6.503360	-0.036486	3.277707
184.201515	3595.997564	6.508365	-0.036578	3.281188
184.174663	3604.003295	6.513370	-0.036578	3.284629
184.548463	3612.031487	6.518374	-0.036653	3.288091
184.793555	3620.106846	6.523379	-0.036704	3.291565
184.656655	3628.158086	6.528384	-0.036684	3.295010
184.810377	3636.215747	6.533389	-0.036718	3.298465
185.025751	3644.211424	6.538394	-0.036763	3.301893
185.293511	3652.202805	6.543398	-0.036818	3.305317
185.494378	3660.275167	6.548403	-0.036861	3.308770
185.860819	3668.276157	6.553408	-0.036934	3.312195
186.307992	3676.321735	6.558413	-0.037023	3.315638
186.374140	3684.332479	6.563418	-0.037040	3.319048
186.606154	3692.342020	6.568422	-0.037089	3.322461
187.015601	3700.346509	6.573427	-0.037170	3.325875
186.898234	3708.389474	6.578432	-0.037154	3.329281
187.268642	3716.447295	6.583437	-0.037228	3.332709
187.698471	3724.470765	6.588442	-0.037313	3.336121
187.748199	3732.487049	6.593446	-0.037328	3.339512
187.885118	3740.543860	6.598451	-0.037358	3.342920
187.856244	3748.588566	6.603456	-0.037358	3.346313
188.561227	3756.587494	6.608461	-0.037495	3.349711
188.679265	3764.645616	6.613466	-0.037522	3.353108
189.010480	3772.658691	6.618470	-0.037589	3.356491
189.249333	3780.660457	6.623475	-0.037639	3.359862
189.512114	3788.655678	6.628480	-0.037693	3.363228
189.818051	3796.723867	6.633485	-0.037755	3.366622
190.108130	3804.734606	6.638490	-0.037814	3.369989
190.307433	3812.778404	6.643494	-0.037857	3.373362
190.582016	3820.837401	6.648499	-0.037913	3.376742
190.932039	3828.828658	6.653504	-0.037984	3.380092
191.279738	3836.862647	6.658509	-0.038054	3.383456
191.247425	3844.912929	6.663514	-0.038053	3.386811
191.330470	3852.946460	6.668518	-0.038074	3.390159
191.996989	3861.059050	6.673523	-0.038203	3.393558
192.338378	3869.032254	6.678528	-0.038272	3.396883
192.467002	3877.052311	6.683533	-0.038301	3.400217
192.780800	3885.033970	6.688538	-0.038365	3.403539
192.852327	3893.072407	6.693542	-0.038383	3.406872
193.039457	3901.098586	6.698547	-0.038423	3.410201
193.233463	3909.106454	6.703552	-0.038465	3.413520
193.801823	3917.138874	6.708557	-0.038576	3.416858
194.074405	3925.137238	6.713562	-0.038632	3.420168
194.130724	3933.168110	6.718566	-0.038647	3.423482
194.257290	3941.237420	6.723571	-0.038676	3.426810
194.582404	3949.227029	6.728576	-0.038742	3.430109
194.751273	3957.317033	6.733581	-0.038779	3.433441
195.043498	3965.335719	6.738586	-0.038838	3.436744
195.186098	3973.315064	6.743590	-0.038870	3.440023
195.426878	3981.364986	6.748595	-0.038920	3.443331
195.679379	3989.378348	6.753600	-0.038973	3.446622
196.159001	3997.381912	6.758605	-0.039067	3.449912
196.213466	4005.455878	6.763610	-0.039082	3.453214
196.187599	4013.509644	6.768614	-0.039083	3.456502
196.597397	4021.488672	6.773619	-0.039164	3.459771
196.929331	4029.487036	6.778624	-0.039231	3.463042
196.833641	4037.587077	6.783629	-0.039219	3.466337
197.000526	4045.574075	6.788634	-0.039255	3.469592
197.469893	4053.622258	6.793638	-0.039348	3.472878
197.794535	4061.682830	6.798643	-0.039414	3.476162
197.853872	4069.615071	6.803648	-0.039430	3.479381
198.276153	4077.676369	6.808653	-0.039514	3.482662
198.448585	4085.661746	6.813658	-0.039551	3.485901
198.634284	4093.711506	6.818662	-0.039591	3.489163
199.006214	4101.749685	6.823667	-0.039665	3.492423
199.186263	4109.763341	6.828672	-0.039704	3.495665
199.447914	4117.804499	6.833677	-0.039758	3.498916
199.678036	4125.819287	6.838682	-0.039806	3.502154
200.031502	4133.814984	6.843686	-0.039877	3.505384
200.122719	4141.905265	6.848691	-0.039900	3.508641
200.211590	4149.898371	6.853696	-0.039921	3.511856
200.806276	4157.935426	6.858701	-0.040037	3.515102
201.004927	4165.933470	6.863706	-0.040080	3.518316
201.400433	4173.927768	6.868710	-0.040158	3.521532
201.575615	4181.943249	6.873715	-0.040196	3.524747
201.777973	4190.008573	6.878720	-0.040239	3.527979
202.103492	4198.069704	6.883725	-0.040305	3.531211
202.246437	4206.107608	6.888730	-0.040337	3.534425
202.434793	4214.120503	6.893734	-0.040377	3.537627
202.643709	4222.146256	6.898739	-0.040422	3.540832
202.676767	4230.142392	6.903744	-0.040433	3.544017
203.078342	4238.202924	6.908749	-0.040513	3.547236
203.254141	4246.232834	6.913754	-0.040551	3.550433
203.545591	4254.334596	6.918758	-0.040611	3.553659
203.829542	4262.389312	6.923763	-0.040669	3.556863
204.063090	4270.293634	6.928768	-0.040717	3.560003
204.198274	4278.310901	6.933773	-0.040748	3.563182
204.475881	4286.355680	6.938778	-0.040805	3.566373
204.653042	4294.336968	6.943782	-0.040843	3.569534
204.813316	4302.423922	6.948787	-0.040878	3.572732
204.852831	4310.439183	6.953792	-0.040891	3.575897
205.146985	4318.438235	6.958797	-0.040951	3.579059
205.505404	4326.429518	6.963802	-0.041023	3.582217
205.483956	4334.459560	6.968806	-0.041024	3.585377
205.699916	4342.504917	6.973811	-0.041069	3.588547
205.912980	4350.524311	6.978816	-0.041114	3.591703
206.332244	4358.564664	6.983821	-0.041198	3.594871
206.445883	4366.580891	6.988826	-0.041224	3.598018
206.788853	4374.581395	6.993830	-0.041293	3.601163
207.051819	4382.587587	6.998835	-0.041347	3.604304
206.919630	4390.629032	7.003840	-0.041328	3.607446
207.282023	4398.648702	7.008845	-0.041401	3.610590
207.408933	4406.694611	7.013850	-0.041430	3.613735
207.417258	4414.739958	7.018854	-0.041436	3.616874
207.897062	4422.747877	7.023859	-0.041531	3.620009
207.862046	4430.751000	7.028864	-0.041530	3.623124
208.249547	4438.794019	7.033869	-0.041607	3.626265
208.337731	4446.804040	7.038874	-0.041629	3.629381
208.542502	4454.853881	7.043878	-0.041672	3.632513
208.947891	4462.920979	7.048883	-0.041753	3.635655
208.931464	4470.860139	7.053888	-0.041755	3.638733
209.154018	4478.922534	7.058893	-0.041802	3.641862
209.541204	4486.891068	7.063898	-0.041879	3.644957
209.784318	4494.914406	7.068902	-0.041930	3.648067
210.092119	4502.988772	7.073907	-0.041992	3.651195
210.132191	4511.013257	7.078912	-0.042005	3.654294
210.164210	4519.085611	7.083917	-0.042016	3.657409
209.986096	4527.100533	7.088922	-0.041988	3.660494
210.229788	4535.070875	7.093926	-0.042039	3.663569
210.632586	4543.129824	7.098931	-0.042119	3.666681
210.696168	4551.095154	7.103936	-0.042136	3.669745
210.776515	4559.203465	7.108941	-0.042156	3.672861
211.023926	4567.192780	7.113946	-0.042208	3.675934
211.127628	4575.188714	7.118950	-0.042232	3.679003
211.442419	4583.238468	7.123955	-0.042296	3.682095
211.742325	4591.169669	7.128960	-0.042357	3.685139
211.908875	4599.241316	7.133965	-0.042393	3.688231
212.033271	4607.324233	7.138970	-0.042422	3.691323
212.121345	4615.346857	7.143974	-0.042443	3.694389
212.481817	4623.354239	7.148979	-0.042516	3.697453
212.615769	4631.311963	7.153984	-0.042546	3.700490
212.849253	4639.361636	7.158989	-0.042595	3.703562
213.059671	4647.399907	7.163994	-0.042639	3.706627
213.149866	4655.377981	7.168998	-0.042661	3.709663
213.434293	4663.521066	7.174003	-0.042719	3.712764
213.782491	4671.543585	7.179008	-0.042790	3.715819
214.008128	4679.541213	7.184013	-0.042837	3.718858
214.283632	4687.524169	7.189018	-0.042893	3.721890
214.184923	4695.506304	7.194022	-0.042880	3.724911
215.021454	4703.548464	7.199027	-0.043041	3.727974
215.187907	4711.546765	7.204032	-0.043077	3.731002
215.622071	4719.607474	7.209037	-0.043163	3.734058
215.715974	4727.630236	7.214042	-0.043186	3.737088
216.042888	4735.606824	7.219046	-0.043252	3.740104
216.480720	4743.645213	7.224051	-0.043339	3.743144
216.503989	4751.668944	7.229056	-0.043349	3.746166
216.794973	4759.724013	7.234061	-0.043408	3.749203
216.858780	4767.789877	7.239066	-0.043425	3.752237
217.110391	4775.784166	7.244070	-0.043477	3.755245
217.304395	4783.837635	7.249075	-0.043519	3.758272
217.148209	4791.845092	7.254080	-0.043495	3.761272
217.498145	4799.831201	7.259085	-0.043565	3.764272
217.845202	4807.869064	7.264090	-0.043635	3.767290
217.985274	4815.881886	7.269094	-0.043666	3.770291
218.268751	4823.963476	7.274099	-0.043725	3.773318
218.327159	4831.977504	7.279104	-0.043741	3.776313
218.527943	4839.965071	7.284109	-0.043783	3.779298
218.618945	4847.970673	7.289114	-0.043805	3.782286
218.614492	4855.950651	7.294118	-0.043810	3.785259
219.138538	4864.027821	7.299123	-0.043913	3.788278
219.240906	4872.041904	7.304128	-0.043937	3.791262
219.466545	4880.106290	7.309133	-0.043984	3.794264
219.727610	4888.101921	7.314138	-0.044038	3.797240
220.043275	4896.081371	7.319142	-0.044102	3.800208
220.356265	4904.091785	7.324147	-0.044166	3.803186
220.480535	4912.098597	7.329152	-0.044194	3.806156
220.901972	4920.128125	7.334157	-0.044278	3.809138
221.140794	4928.146054	7.339162	-0.044327	3.812109
221.028374	4936.209294	7.344166	-0.044312	3.815088
221.452987	4944.252000	7.349171	-0.044396	3.818068
221.454000	4952.241796	7.354176	-0.044402	3.821017
221.726219	4960.231527	7.359181	-0.044457	3.823969
221.737467	4968.284007	7.364186	-0.044465	3.826937
222.004807	4976.267938	7.369190	-0.044520	3.829882
222.298533	4984.333033	7.374195	-0.044580	3.832856
222.653061	4992.362009	7.379200	-0.044651	3.835816
223.019398	5000.332920	7.384205	-0.044724	3.838751
223.158880	5008.409631	7.389210	-0.044756	3.841719
223.167295	5016.343329	7.394214	-0.044762	3.844630
223.477481	5024.428956	7.399219	-0.044826	3.847600
223.715826	5032.426048	7.404224	-0.044875	3.850533
223.754035	5040.484819	7.409229	-0.044888	3.853483
224.014312	5048.533254	7.414234	-0.044941	3.856432
224.278887	5056.498839	7.419238	-0.044996	3.859348
224.722951	5064.553109	7.424243	-0.045084	3.862297
225.019100	5072.547341	7.429248	-0.045144	3.865220
225.340711	5080.579784	7.434253	-0.045209	3.868154
225.545804	5088.638512	7.439258	-0.045253	3.871094
225.760295	5096.856541	7.444262	-0.045298	3.874090
226.066274	5104.841682	7.449267	-0.045360	3.877000
226.260235	5112.712651	7.454272	-0.045401	3.879864
226.347059	5120.751769	7.459277	-0.045423	3.882786
226.615161	5128.720199	7.464282	-0.045478	3.885683
226.861534	5136.713937	7.469286	-0.045529	3.888586
227.004863	5144.799372	7.474291	-0.045561	3.891519
227.270082	5152.790531	7.479296	-0.045616	3.894417
227.580613	5160.777616	7.484301	-0.045679	3.897313
227.711666	5168.822498	7.489306	-0.045708	3.900224
227.719448	5176.824549	7.494310	-0.045715	3.903115
227.923087	5184.879475	7.499315	-0.045758	3.906026
228.091255	5192.881734	7.504320	-0.045795	3.908916
228.238440	5200.928333	7.509325	-0.045827	3.911819
228.297500	5208.950818	7.514330	-0.045844	3.914710
228.611335	5216.959296	7.519334	-0.045907	3.917598
228.850897	5224.968056	7.524339	-0.045957	3.920483
229.133604	5232.955433	7.529344	-0.046015	3.923358
229.318477	5241.005055	7.534349	-0.046055	3.926252
229.709589	5248.985912	7.539354	-0.046133	3.929123
229.751063	5257.010351	7.544358	-0.046146	3.932002
229.839793	5265.088887	7.549363	-0.046168	3.934898
230.100294	5273.073284	7.554368	-0.046221	3.937761
230.127625	5281.081281	7.559373	-0.046232	3.940627
230.187965	5289.090002	7.564378	-0.046248	3.943492
230.463537	5297.109726	7.569382	-0.046305	3.946362
230.712495	5305.135843	7.574387	-0.046356	3.949231
230.677064	5313.194045	7.579392	-0.046355	3.952105
231.048157	5321.235718	7.584397	-0.046429	3.954979
231.465001	5329.222449	7.589402	-0.046512	3.957831
231.508340	5337.200670	7.594406	-0.046525	3.960672
231.879630	5345.223333	7.599411	-0.046600	3.963532
231.993528	5353.237027	7.604416	-0.046626	3.966382
232.171068	5361.256148	7.609421	-0.046665	3.969233
232.340948	5369.315797	7.614426	-0.046701	3.972097
232.492508	5377.324971	7.619430	-0.046735	3.974940
232.708732	5385.414454	7.624435	-0.046780	3.977811
232.812105	5393.381129	7.629440	-0.046805	3.980634
232.938086	5401.378046	7.634445	-0.046834	3.983466
233.117784	5409.387051	7.639450	-0.046872	3.986302
233.420006	5417.405009	7.644454	-0.046934	3.989140
233.593734	5425.502829	7.649459	-0.046971	3.992003
233.615968	5433.515258	7.654464	-0.046981	3.994831
233.903717	5441.529223	7.659469	-0.047040	3.997661
234.126940	5449.512936	7.664474	-0.047086	4.000478
234.205734	5457.540846	7.669478	-0.047106	4.003307
234.511204	5465.558927	7.674483	-0.047169	4.006133
234.416738	5473.590106	7.679488	-0.047156	4.008956
234.849070	5481.620249	7.684493	-0.047242	4.011784
235.203123	5489.680190	7.689498	-0.047313	4.014620
235.114443	5497.674820	7.694502	-0.047302	4.017424
235.470366	5505.657171	7.699507	-0.047373	4.020228
235.778784	5513.671405	7.704512	-0.047436	4.023041
236.140356	5521.671221	7.709517	-0.047509	4.025848
236.228802	5529.748471	7.714522	-0.047530	4.028675
236.438111	5537.740457	7.719526	-0.047575	4.031473
236.715966	5545.879036	7.724531	-0.047632	4.034321
236.872726	5553.847118	7.729536	-0.047666	4.037105
237.074053	5561.799177	7.734541	-0.047709	4.039883
237.507479	5569.823951	7.739546	-0.047795	4.042688
237.618120	5577.809901	7.744550	-0.047820	4.045472
237.851760	5585.856313	7.749555	-0.047869	4.048277
238.167002	5593.829591	7.754560	-0.047933	4.051056
238.307263	5601.908308	7.759565	-0.047965	4.053867
238.541271	5609.932174	7.764570	-0.048013	4.056658
238.671664	5617.888608	7.769574	-0.048043	4.059423
239.029092	5625.957283	7.774579	-0.048115	4.062228
238.993865	5633.934303	7.779584	-0.048113	4.064993
239.191773	5641.980240	7.784589	-0.048155	4.067784
239.440809	5649.999051	7.789594	-0.048207	4.070564
239.669598	5658.024274	7.794598	-0.048255	4.073344
239.917043	5666.078718	7.799603	-0.048306	4.076133
239.802335	5674.032175	7.804608	-0.048290	4.078879
240.132755	5682.092604	7.809613	-0.048357	4.081667
240.257139	5690.029292	7.814618	-0.048385	4.084408
240.386850	5698.083457	7.819622	-0.048415	4.087187
240.645110	5706.131778	7.824627	-0.048468	4.089964
240.892554	5714.148924	7.829632	-0.048519	4.092728
240.951514	5722.192537	7.834637	-0.048536	4.095497
241.323328	5730.200470	7.839642	-0.048610	4.098256
241.404686	5738.206959	7.844646	-0.048630	4.101009
241.676784	5746.216115	7.849651	-0.048686	4.103763
241.821742	5754.232883	7.854656	-0.048719	4.106516
242.231102	5762.239620	7.859661	-0.048800	4.109268
242.271996	5770.325015	7.864666	-0.048813	4.112039
242.532892	5778.353844	7.869670	-0.048867	4.114793
242.953577	5786.358484	7.874675	-0.048950	4.117538
243.009862	5794.305470	7.879680	-0.048966	4.120257
243.346106	5802.363439	7.884685	-0.049034	4.123015
243.627696	5810.363130	7.889690	-0.049092	4.125752
243.660360	5818.374600	7.894694	-0.049103	4.128487
243.880296	5826.444109	7.899699	-0.049149	4.131242
243.993427	5834.459751	7.904704	-0.049175	4.133976
244.147546	5842.493949	7.909709	-0.049209	4.136715
244.413143	5850.489195	7.914714	-0.049264	4.139440
244.306528	5858.540692	7.919718	-0.049249	4.142178
244.727888	5866.517275	7.924723	-0.049333	4.144895
244.757077	5874.563612	7.929728	-0.049344	4.147630
245.039906	5882.545707	7.934733	-0.049402	4.150343
245.301654	5890.630523	7.939738	-0.049456	4.153090
245.291265	5898.637192	7.944742	-0.049459	4.155805
245.601911	5906.643596	7.949747	-0.049522	4.158521
245.608364	5914.636256	7.954752	-0.049529	4.161228
245.950996	5922.628243	7.959757	-0.049598	4.163937
245.999148	5930.698324	7.964762	-0.049612	4.166667
245.869844	5938.675272	7.969766	-0.049593	4.169361
246.476645	5946.746478	7.974771	-0.049711	4.172094
246.495817	5954.735418	7.979776	-0.049720	4.174791
246.430286	5962.770295	7.984781	-0.049713	4.177501
246.711737	5970.757292	7.989786	-0.049771	4.180196
246.836904	5978.754666	7.994790	-0.049799	4.182892
247.015355	5986.798201	7.999795	-0.049838	4.185602
247.074590	5994.837877	8.004800	-0.049854	4.188307
247.307661	6002.814981	8.009805	-0.049903	4.190992
247.823674	6010.963962	8.014810	-0.050004	4.193735
247.703076	6018.968440	8.019814	-0.049987	4.196422
248.046108	6026.838717	8.024819	-0.050056	4.199066
248.120947	6034.926430	8.029824	-0.050075	4.201780
248.418976	6042.854991	8.034829	-0.050136	4.204440
248.482691	6050.939533	8.039834	-0.050153	4.207148
248.502801	6058.907492	8.044838	-0.050162	4.209815
248.491214	6066.986988	8.049843	-0.050165	4.212518
248.694484	6075.012851	8.054848	-0.050208	4.215203
249.122082	6082.981081	8.059853	-0.050293	4.217869
249.286180	6091.023215	8.064858	-0.050329	4.220555
249.252620	6098.988429	8.069862	-0.050328	4.223212
249.746992	6106.988036	8.074867	-0.050425	4.225884
250.057458	6115.031109	8.079872	-0.050488	4.228568
250.152955	6123.084746	8.084877	-0.050511	4.231250
250.308012	6131.172788	8.089882	-0.050545	4.233943
250.326957	6139.136614	8.094886	-0.050554	4.236592
250.764552	6147.190279	8.099891	-0.050641	4.239273
250.829652	6155.163877	8.104896	-0.050658	4.241922
251.146220	6163.117542	8.109901	-0.050722	4.244565
251.405892	6171.196509	8.114906	-0.050776	4.247247
251.424180	6179.153628	8.119910	-0.050784	4.249886
251.698727	6187.256636	8.124915	-0.050841	4.252573
251.909623	6195.296832	8.129920	-0.050885	4.255237
251.851538	6203.285286	8.134925	-0.050880	4.257879
251.964564	6211.323182	8.139930	-0.050906	4.260538
252.154465	6219.298890	8.144934	-0.050947	4.263176
252.423426	6227.358840	8.149939	-0.051002	4.265840
252.724035	6235.336063	8.154944	-0.051063	4.268476
252.999608	6243.407998	8.159949	-0.051120	4.271141
253.240286	6251.434843	8.164954	-0.051170	4.273789
253.221108	6259.504758	8.169958	-0.051172	4.276447
253.476090	6267.434187	8.174963	-0.051224	4.279060
253.744656	6275.442259	8.179968	-0.051280	4.281697
253.822403	6283.425056	8.184973	-0.051299	4.284323
253.888706	6291.533765	8.189978	-0.051317	4.286988
254.356919	6299.447397	8.194982	-0.051409	4.289591
254.666356	6307.529793	8.199987	-0.051472	4.292246
254.611538	6315.572909	8.204992	-0.051467	4.294884
254.941265	6323.554475	8.209997	-0.051534	4.297503
255.272463	6331.564846	8.215002	-0.051601	4.300130
255.252975	6339.596250	8.220006	-0.051602	4.302759
255.407847	6347.579766	8.225011	-0.051636	4.305373
255.456534	6355.631816	8.230016	-0.051651	4.308006
255.882885	6363.604540	8.235021	-0.051735	4.310615
255.856648	6371.722758	8.240026	-0.051736	4.313266
255.911547	6379.706334	8.245030	-0.051751	4.315872
256.071647	6387.693337	8.250035	-0.051786	4.318479
256.300291	6395.745005	8.255040	-0.051834	4.321105
256.552440	6403.712962	8.260045	-0.051886	4.323703
256.572821	6411.753284	8.265050	-0.051895	4.326321
256.674030	6419.746817	8.270054	-0.051919	4.328923
256.947204	6427.785648	8.275059	-0.051975	4.331539
257.086719	6435.800624	8.280064	-0.052007	4.334145
257.156495	6443.845048	8.285069	-0.052025	4.336759
257.303903	6451.820568	8.290074	-0.052058	4.339349
257.665179	6459.830136	8.295078	-0.052130	4.341950
257.978154	6467.822543	8.300083	-0.052194	4.344543
257.976175	6475.881263	8.305088	-0.052199	4.347154
258.318190	6483.862618	8.310093	-0.052267	4.349741
258.815376	6491.986627	8.315098	-0.052365	4.352374
258.861204	6500.024350	8.320102	-0.052379	4.354974
258.790894	6508.010263	8.325107	-0.052371	4.357555
259.082723	6515.943539	8.330112	-0.052431	4.360119
259.319518	6523.979402	8.335117	-0.052480	4.362715
259.570558	6531.964714	8.340122	-0.052532	4.365293
259.473013	6539.984711	8.345126	-0.052519	4.367879
259.922986	6547.997208	8.350131	-0.052608	4.370464
259.934501	6556.055752	8.355136	-0.052616	4.373060
260.025343	6564.032263	8.360141	-0.052638	4.375628
260.567450	6572.061595	8.365146	-0.052744	4.378214
260.495865	6580.067123	8.370150	-0.052736	4.380788
260.519019	6588.108694	8.375155	-0.052745	4.383372
260.799995	6596.103808	8.380160	-0.052803	4.385941
261.185117	6604.141811	8.385165	-0.052880	4.388523
261.255059	6612.176507	8.390170	-0.052898	4.391100
261.130177	6620.199793	8.395174	-0.052880	4.393672
261.340781	6628.225988	8.400179	-0.052925	4.396244
261.362698	6636.186965	8.405184	-0.052934	4.398793
261.628872	6644.211994	8.410189	-0.052989	4.401363
261.980590	6652.213094	8.415194	-0.053059	4.403923
262.267573	6660.221015	8.420198	-0.053118	4.406484
262.471860	6668.240894	8.425203	-0.053161	4.409047
262.524480	6676.321706	8.430208	-0.053177	4.411627
262.809203	6684.324406	8.435213	-0.053235	4.414182
262.938400	6692.375371	8.440218	-0.053264	4.416750
263.040764	6700.338391	8.445222	-0.053288	4.419288
263.449601	6708.412273	8.450227	-0.053370	4.421861
263.573382	6716.394165	8.455232	-0.053398	4.424403
263.572998	6724.431585	8.460237	-0.053403	4.426960
263.673679	6732.448641	8.465242	-0.053427	4.429509
263.838157	6740.472412	8.470246	-0.053463	4.432059
263.996511	6748.531447	8.475251	-0.053498	4.434619
264.346516	6756.527642	8.480256	-0.053568	4.437159
264.665719	6764.462034	8.485261	-0.053633	4.439677
264.902103	6772.585393	8.490266	-0.053682	4.442253
264.980356	6780.453463	8.495270	-0.053702	4.444747
265.037276	6788.518573	8.500275	-0.053718	4.447301
265.057088	6796.564154	8.505280	-0.053727	4.449847
265.125331	6804.612765	8.510285	-0.053745	4.452393
265.414346	6812.646496	8.515290	-0.053804	4.454934
265.609621	6820.591181	8.520294	-0.053845	4.457444
265.839370	6828.619141	8.525299	-0.053893	4.459980
265.660912	6836.657560	8.530304	-0.053865	4.462516
265.966649	6844.591909	8.535309	-0.053928	4.465020
266.057442	6852.679913	8.540314	-0.053950	4.467569
266.003748	6860.671102	8.545318	-0.053945	4.470087
266.407291	6868.753009	8.550323	-0.054025	4.472633
266.530058	6876.770272	8.555328	-0.054053	4.475156
266.690490	6884.766891	8.560333	-0.054089	4.477671
267.071165	6892.750884	8.565338	-0.054165	4.480182
267.058301	6900.768383	8.570343	-0.054168	4.482700
267.213365	6908.756882	8.575347	-0.054202	4.485209
267.366072	6916.812646	8.580352	-0.054235	4.487737
267.758770	6924.797022	8.585357	-0.054314	4.490242
268.051951	6932.845744	8.590362	-0.054374	4.492766
267.919168	6940.836251	8.595367	-0.054354	4.495268
268.373805	6948.908651	8.600371	-0.054444	4.497797
268.509183	6956.862847	8.605376	-0.054474	4.500286
268.786350	6964.846246	8.610381	-0.054531	4.502783
268.951274	6972.892095	8.615386	-0.054567	4.505298
268.935085	6980.894022	8.620391	-0.054569	4.507798
269.377671	6988.958712	8.625395	-0.054657	4.510317
269.372772	6997.028610	8.630400	-0.054661	4.512835
269.502812	7005.070942	8.635405	-0.054691	4.515343
269.859450	7013.066010	8.640410	-0.054763	4.517835
269.593761	7020.996987	8.645415	-0.054718	4.520305
269.958312	7029.014004	8.650419	-0.054791	4.522802
270.204169	7036.983225	8.655424	-0.054842	4.525282
270.211124	7045.056938	8.660429	-0.054849	4.527793
270.410721	7053.039439	8.665434	-0.054891	4.530274
270.654458	7061.060306	8.670439	-0.054942	4.532766
271.009201	7069.110160	8.675443	-0.055013	4.535266
271.103439	7077.126892	8.680448	-0.055036	4.537754
271.140331	7085.113150	8.685453	-0.055048	4.540230
271.463481	7093.117322	8.690458	-0.055114	4.542712
271.337760	7101.133440	8.695463	-0.055095	4.545195
271.591234	7109.156994	8.700467	-0.055148	4.547679
271.701072	7117.177680	8.705472	-0.055174	4.550161
271.847297	7125.206662	8.710477	-0.055206	4.552644
272.264646	7133.281293	8.715482	-0.055289	4.555141
272.267951	7141.222825	8.720487	-0.055295	4.557594
272.496860	7149.243564	8.725491	-0.055343	4.560071
272.693640	7157.274960	8.730496	-0.055385	4.562549
272.838075	7165.223926	8.735501	-0.055417	4.565001
273.136353	7173.313449	8.740506	-0.055478	4.567495
272.940211	7181.322015	8.745511	-0.055446	4.569962
273.288254	7189.384829	8.750515	-0.055516	4.572445
273.352868	7197.392133	8.755520	-0.055534	4.574909
273.398253	7205.406886	8.760525	-0.055547	4.577374
273.628055	7213.389949	8.765530	-0.055595	4.579828
273.832801	7221.413027	8.770535	-0.055639	4.582293
274.041462	7229.380502	8.775539	-0.055683	4.584740
274.202147	7237.462313	8.780544	-0.055718	4.587220
274.332053	7245.468196	8.785549	-0.055747	4.589676
274.674915	7253.521880	8.790554	-0.055816	4.592145
274.566359	7261.543998	8.795559	-0.055802	4.594603
274.809199	7269.596454	8.800563	-0.055852	4.597069
274.888413	7277.526992	8.805568	-0.055872	4.599497
275.149456	7285.558582	8.810573	-0.055926	4.601954
275.246951	7293.512970	8.815578	-0.055949	4.604386
275.512190	7301.580879	8.820583	-0.056004	4.606851
275.618211	7309.569419	8.825587	-0.056029	4.609291
275.930750	7317.611332	8.830592	-0.056092	4.611746
276.039843	7325.650470	8.835597	-0.056118	4.614199
276.117784	7333.712359	8.840602	-0.056138	4.616657
276.112238	7341.645334	8.845607	-0.056142	4.619075
276.295268	7349.637964	8.850611	-0.056181	4.621509
276.469874	7357.694375	8.855616	-0.056219	4.623962
276.428010	7365.689218	8.860621	-0.056216	4.626394
276.842564	7373.768944	8.865626	-0.056299	4.628851
276.975226	7381.728397	8.870631	-0.056329	4.631271
277.189501	7389.790892	8.875635	-0.056374	4.633720
277.287185	7397.811243	8.880640	-0.056397	4.636155
277.443664	7405.747480	8.885645	-0.056432	4.638563
277.759282	7413.777844	8.890650	-0.056496	4.640999
277.762941	7421.782946	8.895655	-0.056502	4.643426
277.912105	7429.802937	8.900659	-0.056535	4.645855
278.207871	7437.801831	8.905664	-0.056595	4.648277
278.191362	7445.857719	8.910669	-0.056597	4.650716
278.652386	7453.901835	8.915674	-0.056688	4.653149
278.505872	7461.878027	8.920679	-0.056666	4.655560
278.817987	7469.876505	8.925683	-0.056729	4.657977
278.917432	7477.924979	8.930688	-0.056753	4.660408
278.866901	7485.910892	8.935693	-0.056749	4.662819
279.336614	7493.912434	8.940698	-0.056842	4.665232
279.379289	7501.945422	8.945703	-0.056855	4.667655
279.576527	7509.965705	8.950707	-0.056897	4.670072
279.701924	7518.039642	8.955712	-0.056926	4.672504
279.854854	7526.106571	8.960717	-0.056959	4.674932
279.943312	7534.120352	8.965722	-0.056981	4.677344
279.968691	7542.042451	8.970727	-0.056991	4.679727
280.268627	7550.069861	8.975731	-0.057052	4.682139
280.459798	7557.996973	8.980736	-0.057093	4.684521
280.447887	7566.064252	8.985741	-0.057096	4.686943
280.795671	7574.089025	8.990746	-0.057166	4.689351
280.858291	7582.074614	8.995751	-0.057183	4.691747
281.029450	7590.150429	9.000755	-0.057220	4.694168
281.329021	7598.169875	9.005760	-0.057281	4.696571
281.454203	7606.118318	9.010765	-0.057309	4.698951
281.463156	7614.189975	9.015770	-0.057316	4.701368
281.541581	7622.158810	9.020775	-0.057336	4.703752
281.834981	7630.182420	9.025779	-0.057396	4.706151
282.149871	7638.218769	9.030784	-0.057460	4.708552
282.141518	7646.227524	9.035789	-0.057464	4.710945
282.329521	7654.251361	9.040794	-0.057504	4.713341
282.450127	7662.294495	9.045799	-0.057532	4.715741
282.620819	7670.294051	9.050803	-0.057569	4.718127
282.901400	7678.297638	9.055808	-0.057626	4.720512
283.198990	7686.313924	9.060813	-0.057687	4.722900
283.374262	7694.337472	9.065818	-0.057725	4.725289
283.462172	7702.343366	9.070823	-0.057746	4.727672
283.717001	7710.353873	9.075827	-0.057799	4.730055
283.736494	7718.393550	9.080832	-0.057808	4.732446
283.788377	7726.370390	9.085837	-0.057823	4.734817
284.272243	7734.490149	9.090842	-0.057918	4.737228
284.266965	7742.398883	9.095847	-0.057922	4.739576
284.431103	7750.452208	9.100851	-0.057958	4.741966
284.485935	7758.447444	9.105856	-0.057974	4.744337
284.695840	7766.486307	9.110861	-0.058018	4.746720
284.901834	7774.519772	9.115866	-0.058061	4.749100
284.934937	7782.480552	9.120871	-0.058073	4.751457
285.262149	7790.566814	9.125875	-0.058139	4.753850
285.594749	7798.618297	9.130880	-0.058206	4.756231
285.354054	7806.526734	9.135885	-0.058167	4.758571
285.761429	7814.591499	9.140890	-0.058248	4.760953
285.865612	7822.536269	9.145895	-0.058272	4.763300
285.832127	7830.577417	9.150899	-0.058271	4.765675
286.144500	7838.606824	9.155904	-0.058335	4.768043
286.232950	7846.600437	9.160909	-0.058356	4.770401
286.507954	7854.685199	9.165914	-0.058413	4.772784
286.610418	7862.679650	9.170919	-0.058437	4.775139
286.877206	7870.686654	9.175923	-0.058492	4.777497
286.970248	7878.700670	9.180928	-0.058515	4.779856
288.015154	7886.692527	9.185933	-0.058715	4.782203
288.811700	7894.691624	9.190938	-0.058868	4.784553
289.375194	7902.740534	9.195943	-0.058978	4.786916
289.630884	7910.714824	9.200947	-0.059031	4.789258
289.855275	7918.813894	9.205952	-0.059078	4.791635
290.122590	7926.767700	9.210957	-0.059133	4.793969
290.395076	7934.853304	9.215962	-0.059189	4.796340
290.428019	7942.770059	9.220967	-0.059201	4.798661
290.787547	7950.815014	9.225971	-0.059273	4.801017
291.022416	7958.839743	9.230976	-0.059322	4.803367
291.151188	7966.832700	9.235981	-0.059351	4.805706
291.208497	7974.869021	9.240986	-0.059367	4.808058
291.399777	7982.899721	9.245991	-0.059408	4.810406
291.474390	7990.400593	9.250995	-0.059427	4.812598
291.679448	7995.138535	9.256000	-0.059468	4.813982
291.841207	7997.568853	9.261005	-0.059500	4.814691
292.187217	7998.922118	9.266010	-0.059565	4.815085
292.154800	7999.666476	9.271015	-0.059559	4.815303
292.138224	7999.680097	9.276019	-0.059556	4.815307
292.427590	8000.001234	9.281024	-0.059610	4.815399
292.298922	8000.258819	9.286029	-0.059587	4.815475
292.486609	8000.079165	9.291034	-0.059621	4.815422
292.532356	8000.146188	9.296039	-0.059630	4.815441
292.613752	8000.214870	9.301043	-0.059645	4.815461
292.781620	7999.971830	9.306048	-0.059676	4.815389
292.763034	8000.147873	9.311053	-0.059673	4.815440
293.186519	7999.979602	9.316058	-0.059752	4.815389
293.011378	8000.266347	9.321063	-0.059719	4.815474
292.815312	8000.273791	9.326067	-0.059683	4.815477
292.958230	8000.078432	9.331072	-0.059709	4.815419
293.010301	8000.396728	9.336077	-0.059719	4.815512
293.183745	8000.065067	9.341082	-0.059751	4.815414
293.259595	8000.221299	9.346087	-0.059766	4.815459
293.304035	8000.070268	9.351091	-0.059774	4.815415
293.259612	8000.255505	9.356096	-0.059766	4.815469
293.255247	8000.208407	9.361101	-0.059765	4.815456
293.251511	8000.101467	9.366106	-0.059764	4.815424
293.312844	8000.213639	9.371111	-0.059776	4.815457
293.459852	8000.174391	9.376115	-0.059803	4.815445
293.683444	8000.110759	9.381120	-0.059845	4.815425
293.623883	8000.182454	9.386125	-0.059834	4.815446
293.524978	8000.155167	9.391130	-0.059815	4.815439
293.755789	8000.109824	9.396135	-0.059858	4.815424
293.737854	8000.137318	9.401139	-0.059855	4.815433
293.786501	8000.146675	9.406144	-0.059864	4.815435
293.950406	8000.055336	9.411149	-0.059894	4.815408
294.106092	8000.029057	9.416154	-0.059923	4.815399
293.701313	8000.146339	9.421159	-0.059848	4.815435
293.732928	8000.089149	9.426163	-0.059854	4.815419
293.917936	8000.008846	9.431168	-0.059888	4.815394
293.808152	8000.148113	9.436173	-0.059868	4.815435
293.832072	8000.036286	9.441178	-0.059873	4.815403
293.970121	8000.116596	9.446183	-0.059898	4.815425
293.814911	8000.053106	9.451187	-0.059869	4.815408
294.045161	8000.063332	9.456192	-0.059912	4.815409
293.851476	8000.146701	9.461197	-0.059876	4.815435
294.103163	8000.117736	9.466202	-0.059923	4.815425
294.098626	8000.097356	9.471207	-0.059922	4.815419
294.241068	8000.052688	9.476211	-0.059949	4.815405
294.368447	7999.977844	9.481216	-0.059972	4.815383
294.179676	8000.131836	9.486221	-0.059937	4.815429
294.215957	8000.051208	9.491226	-0.059944	4.815405
294.293057	8000.037523	9.496231	-0.059959	4.815401
294.262065	8000.172751	9.501235	-0.059953	4.815440
294.228857	8000.020431	9.506240	-0.059947	4.815396
294.055493	8000.009013	9.511245	-0.059914	4.815394
294.295298	7999.976645	9.516250	-0.059959	4.815383
294.257955	8000.047639	9.521255	-0.059952	4.815404
294.069543	8000.113994	9.526259	-0.059917	4.815424
294.202891	8000.077726	9.531264	-0.059942	4.815413
294.296173	8000.096373	9.536269	-0.059959	4.815418
294.264609	7999.991109	9.541274	-0.059953	4.815387
294.440078	8000.016460	9.546279	-0.059986	4.815394
294.473399	7999.995637	9.551283	-0.059992	4.815388
294.617903	7999.998032	9.556288	-0.060019	4.815388
294.662160	7999.966701	9.561293	-0.060027	4.815378
294.503500	7999.975833	9.566298	-0.059998	4.815382
294.479996	8000.082328	9.571303	-0.059994	4.815413
294.422347	8000.109164	9.576307	-0.059983	4.815421
294.555426	7999.970285	9.581312	-0.060008	4.815380
294.567738	8000.136158	9.586317	-0.060010	4.815428
294.498805	7999.981108	9.591322	-0.059997	4.815383
294.555310	7999.990596	9.596327	-0.060008	4.815386
294.716787	8000.091603	9.601331	-0.060038	4.815414
294.523307	8000.018927	9.606336	-0.060002	4.815394
294.370437	8000.290017	9.611341	-0.059974	4.815474
294.766834	8000.016550	9.616346	-0.060047	4.815392
294.675347	8000.167879	9.621351	-0.060030	4.815437
294.516151	8000.060500	9.626355	-0.060001	4.815406
294.507595	8000.028295	9.631360	-0.059999	4.815397
294.703748	8000.206833	9.636365	-0.060036	4.815448
294.656918	8000.084212	9.641370	-0.060027	4.815413
294.890484	8000.135110	9.646375	-0.060070	4.815426
294.950354	7999.976848	9.651379	-0.060081	4.815380
294.910934	7999.990092	9.656384	-0.060074	4.815384
294.761765	8000.169324	9.661389	-0.060047	4.815437
294.996049	7999.842938	9.666394	-0.060090	4.815340
295.196364	7999.985204	9.671399	-0.060127	4.815381
295.098510	7999.949383	9.676403	-0.060109	4.815371
294.925360	8000.049124	9.681408	-0.060077	4.815401
294.986255	8000.099301	9.686413	-0.060088	4.815415
295.014022	7999.936232	9.691418	-0.060093	4.815368
294.694057	7999.983308	9.696423	-0.060034	4.815383
294.799536	7999.997882	9.701427	-0.060054	4.815387
295.034509	8000.013531	9.706432	-0.060097	4.815390
294.769778	8000.133133	9.711437	-0.060048	4.815426
294.905125	7999.997497	9.716442	-0.060073	4.815386
295.033189	8000.026341	9.721447	-0.060097	4.815394
294.915639	8000.123797	9.726451	-0.060075	4.815423
294.995253	7999.997926	9.731456	-0.060090	4.815386
294.971563	8000.232679	9.736461	-0.060086	4.815454
295.057982	8000.064167	9.741466	-0.060102	4.815405
295.074948	7999.955429	9.746471	-0.060105	4.815373
294.851054	7999.957067	9.751475	-0.060063	4.815375
295.251127	7999.876050	9.756480	-0.060138	4.815349
295.014864	7999.878553	9.761485	-0.060094	4.815351
295.236766	7999.983768	9.766490	-0.060135	4.815380
295.203757	8000.066592	9.771495	-0.060129	4.815405
295.013451	7999.962971	9.776499	-0.060094	4.815375
295.179069	7999.958234	9.781504	-0.060125	4.815373
295.370811	8000.139907	9.786509	-0.060160	4.815425
295.329751	7999.932943	9.791514	-0.060153	4.815365
295.090600	8000.012353	9.796519	-0.060108	4.815390
295.251533	7999.998988	9.801523	-0.060138	4.815385
295.247958	7999.876015	9.806528	-0.060137	4.815349
295.049857	7999.993513	9.811533	-0.060101	4.815384
295.051042	7999.857794	9.816538	-0.060101	4.815345
295.419578	8000.029567	9.821543	-0.060170	4.815393
295.118493	8000.109020	9.826547	-0.060114	4.815418
295.174414	7999.978482	9.831552	-0.060124	4.815379
295.148445	7999.996223	9.836557	-0.060119	4.815385
295.185744	8000.028908	9.841562	-0.060126	4.815394
295.139143	8000.170293	9.846567	-0.060118	4.815435
295.172543	8000.044725	9.851571	-0.060124	4.815399
295.330157	7999.999240	9.856576	-0.060153	4.815385
295.219778	8000.203699	9.861581	-0.060133	4.815445
295.238713	7999.959250	9.866586	-0.060136	4.815373
295.345655	8000.169447	9.871591	-0.060156	4.815434
295.262471	8000.029122	9.876595	-0.060140	4.815394
295.198733	7999.954318	9.881600	-0.060129	4.815372
295.313781	8000.153960	9.886605	-0.060150	4.815430
295.375152	7999.993584	9.891610	-0.060162	4.815383
295.401845	8000.017542	9.896615	-0.060167	4.815390
295.482665	7999.966509	9.901619	-0.060182	4.815374
295.537823	7999.979182	9.906624	-0.060192	4.815378
295.317125	8000.033245	9.911629	-0.060151	4.815395
295.525056	7999.885985	9.916634	-0.060189	4.815350
295.489281	8000.002966	9.921639	-0.060183	4.815385
295.576961	8000.005489	9.926643	-0.060199	4.815385
295.532170	7999.779224	9.931648	-0.060191	4.815319
295.523412	7999.991779	9.936653	-0.060189	4.815381
295.652363	7999.984297	9.941658	-0.060213	4.815379
295.392078	7999.986401	9.946663	-0.060165	4.815380
295.165871	7999.975174	9.951667	-0.060123	4.815378
295.263098	7999.884867	9.956672	-0.060141	4.815351
295.236630	8000.029791	9.961677	-0.060136	4.815394
295.483415	8000.001815	9.966682	-0.060182	4.815385
295.430489	8000.034074	9.971687	-0.060172	4.815394
295.492559	7999.928220	9.976691	-0.060184	4.815363
295.432313	7999.926155	9.981696	-0.060172	4.815363
295.247448	8000.019290	9.986701	-0.060138	4.815391
295.432599	8000.160240	9.991706	-0.060173	4.815431
295.608509	8000.156743	9.996711	-0.060205	4.815429
295.590631	7999.906338	10.001715	-0.060202	4.815356
295.472912	7999.872326	10.006720	-0.060180	4.815347
295.273370	8000.214258	10.011725	-0.060143	4.815448
295.393152	7999.989649	10.016730	-0.060165	4.815381
295.534868	8000.040095	10.021735	-0.060192	4.815395
295.658950	7999.859381	10.026739	-0.060215	4.815342
295.657935	7999.873260	10.031744	-0.060215	4.815346
295.701327	7999.999035	10.036749	-0.060223	4.815383
295.732485	7999.982452	10.041754	-0.060229	4.815378
295.676060	8000.003964	10.046759	-0.060218	4.815384
295.488580	7999.968795	10.051763	-0.060183	4.815375
295.756998	7999.882391	10.056768	-0.060233	4.815348
295.795649	8000.015570	10.061773	-0.060240	4.815387
295.783770	7999.974759	10.066778	-0.060238	4.815375
295.866621	7999.874593	10.071783	-0.060254	4.815345
295.670447	7999.913030	10.076787	-0.060217	4.815358
295.833555	7999.862291	10.081792	-0.060248	4.815342
295.754447	7999.882359	10.086797	-0.060233	4.815348
295.859009	7999.792173	10.091802	-0.060252	4.815321
295.596898	7999.971674	10.096807	-0.060204	4.815375
295.627592	7999.885608	10.101811	-0.060209	4.815350
295.880416	7999.905829	10.106816	-0.060256	4.815355
295.688441	7999.987090	10.111821	-0.060221	4.815379
295.594670	7999.870104	10.116826	-0.060203	4.815345
295.645341	7999.974622	10.121831	-0.060213	4.815376
295.918831	7999.921436	10.126835	-0.060264	4.815359
295.890852	7999.862188	10.131840	-0.060258	4.815342
295.666385	7999.945048	10.136845	-0.060217	4.815367
295.632149	7999.974410	10.141850	-0.060210	4.815376
295.808755	7999.869384	10.146855	-0.060243	4.815344
295.722533	8000.103104	10.151859	-0.060227	4.815413
295.835441	8000.001298	10.156864	-0.060248	4.815383
295.829553	8000.164736	10.161869	-0.060247	4.815430
295.729386	7999.996338	10.166874	-0.060229	4.815382
295.613782	8000.001906	10.171879	-0.060207	4.815384
295.646748	8000.112545	10.176883	-0.060213	4.815416
295.775774	7999.971459	10.181888	-0.060237	4.815374
295.776357	7999.985365	10.186893	-0.060237	4.815378
295.797317	7999.880967	10.191898	-0.060241	4.815348
295.893742	7999.989451	10.196903	-0.060259	4.815379
295.811682	8000.007332	10.201907	-0.060244	4.815385
295.903186	7999.860280	10.206912	-0.060261	4.815341
295.789962	8000.024077	10.211917	-0.060240	4.815390
295.961344	7999.884761	10.216922	-0.060272	4.815348
295.855733	7999.864843	10.221927	-0.060252	4.815343
295.705426	7999.890146	10.226931	-0.060224	4.815351
295.920351	7999.885156	10.231936	-0.060264	4.815348
295.666128	8000.041274	10.236941	-0.060217	4.815395
295.982682	8000.019798	10.241946	-0.060276	4.815387
295.934726	8000.009386	10.246951	-0.060267	4.815385
295.760228	7999.992602	10.251955	-0.060235	4.815380
295.970808	8000.016400	10.256960	-0.060274	4.815386
295.722353	7999.984496	10.261965	-0.060228	4.815378
295.870757	8000.047880	10.266970	-0.060255	4.815396
295.968668	8000.001406	10.271975	-0.060273	4.815382
295.790570	8000.002732	10.276979	-0.060240	4.815383
296.084515	7999.876135	10.281984	-0.060295	4.815345
295.874132	8000.134520	10.286989	-0.060256	4.815421
295.974876	7999.877529	10.291994	-0.060275	4.815346
296.030569	7999.901968	10.296999	-0.060285	4.815353
295.858250	8000.071200	10.302003	-0.060253	4.815403
295.828642	7999.938174	10.307008	-0.060247	4.815364
296.011450	8000.052364	10.312013	-0.060282	4.815397
295.991087	7999.987897	10.317018	-0.060278	4.815378
295.909153	7999.872175	10.322023	-0.060262	4.815345
295.851242	7999.988791	10.327027	-0.060252	4.815379
295.964654	7999.929747	10.332032	-0.060273	4.815361
295.869376	7999.989094	10.337037	-0.060255	4.815379
295.967687	7999.977898	10.342042	-0.060274	4.815375
296.001099	7999.961352	10.347047	-0.060280	4.815370
295.941242	8000.012736	10.352051	-0.060269	4.815385
295.952999	7999.887877	10.357056	-0.060271	4.815349
296.005848	8000.141004	10.362061	-0.060281	4.815423
295.991779	7999.887454	10.367066	-0.060278	4.815349
295.892893	7999.877267	10.372071	-0.060260	4.815346
295.930204	7999.996529	10.377075	-0.060267	4.815381
296.226017	7999.875306	10.382080	-0.060322	4.815344
295.963138	7999.952186	10.387085	-0.060273	4.815368
296.174070	7999.980266	10.392090	-0.060312	4.815375
296.011013	7999.868543	10.397095	-0.060282	4.815343
295.971365	8000.029285	10.402099	-0.060274	4.815390
295.936009	7999.966707	10.407104	-0.060268	4.815372
296.042139	7999.967398	10.412109	-0.060288	4.815372
296.088596	7999.973514	10.417114	-0.060296	4.815373
295.856637	7999.876683	10.422119	-0.060253	4.815346
295.955892	7999.977732	10.427123	-0.060272	4.815375
295.926083	7999.865011	10.432128	-0.060266	4.815342
295.884148	7999.997924	10.437133	-0.060258	4.815381
295.881834	7999.851455	10.442138	-0.060258	4.815339
295.983989	8000.022027	10.447143	-0.060277	4.815388
295.755058	8000.078092	10.452147	-0.060234	4.815405
295.874589	7999.827826	10.457152	-0.060257	4.815332
296.008839	7999.915559	10.462157	-0.060282	4.815357
296.200835	7999.874918	10.467162	-0.060317	4.815344
296.192417	7999.788204	10.472167	-0.060316	4.815319
296.121284	7999.887499	10.477171	-0.060303	4.815348
296.233757	7999.887226	10.482176	-0.060324	4.815347
296.016547	7999.917833	10.487181	-0.060283	4.815357
296.214549	7999.964937	10.492186	-0.060320	4.815370
296.361303	7999.863691	10.497191	-0.060347	4.815340
295.994775	8000.092769	10.502195	-0.060279	4.815409
296.219426	7999.988538	10.507200	-0.060321	4.815377
296.138331	7999.962612	10.512205	-0.060306	4.815370
296.325659	7999.960373	10.517210	-0.060341	4.815368
296.157928	7999.889190	10.522215	-0.060310	4.815348
295.938083	8000.043740	10.527219	-0.060269	4.815395
296.084047	7999.831320	10.532224	-0.060296	4.815332
296.116028	8000.058449	10.537229	-0.060302	4.815398
296.088240	7999.922245	10.542234	-0.060297	4.815358
296.128129	7999.941078	10.547239	-0.060304	4.815364
296.012709	8000.141182	10.552243	-0.060283	4.815423
296.092967	8000.003562	10.557248	-0.060298	4.815382
296.123224	8000.079953	10.562253	-0.060303	4.815404
296.236976	7999.983505	10.567258	-0.060325	4.815375
296.243925	7999.945143	10.572263	-0.060326	4.815364
295.948027	7999.987272	10.577267	-0.060271	4.815378
296.059022	7999.877952	10.582272	-0.060291	4.815345
296.083848	8000.113513	10.587277	-0.060296	4.815414
296.001675	7999.991372	10.592282	-0.060281	4.815379
295.956058	7999.956415	10.597287	-0.060272	4.815369
295.996475	8000.026562	10.602291	-0.060280	4.815389
296.039874	7999.880850	10.607296	-0.060288	4.815346
296.016910	7999.908261	10.612301	-0.060284	4.815355
296.063393	7999.959269	10.617306	-0.060292	4.815369
296.132035	7999.959339	10.622311	-0.060305	4.815369
296.092945	8000.043133	10.627315	-0.060298	4.815394
296.422477	7999.936364	10.632320	-0.060359	4.815361
296.382085	8000.130230	10.637325	-0.060352	4.815418
296.337126	7999.937091	10.642330	-0.060343	4.815361
296.079786	7999.988410	10.647335	-0.060296	4.815378
296.238758	7999.966461	10.652339	-0.060325	4.815370
296.096711	7999.870051	10.657344	-0.060299	4.815343
296.071793	8000.021417	10.662349	-0.060294	4.815387
296.280258	7999.975705	10.667354	-0.060333	4.815373
296.298326	8000.113889	10.672359	-0.060336	4.815413
296.115546	7999.881058	10.677363	-0.060302	4.815346
296.314741	7999.901461	10.682368	-0.060339	4.815351
296.153664	8000.054847	10.687373	-0.060310	4.815397
296.161237	7999.860443	10.692378	-0.060311	4.815340
296.350321	7999.977945	10.697383	-0.060346	4.815373
296.349362	7999.878527	10.702387	-0.060346	4.815344
296.184362	8000.007264	10.707392	-0.060315	4.815383
296.073927	8000.063155	10.712397	-0.060295	4.815399
296.131536	7999.914471	10.717402	-0.060305	4.815356
296.160879	7999.885031	10.722407	-0.060311	4.815347
296.204327	7999.979811	10.727411	-0.060319	4.815375
296.264964	7999.789493	10.732416	-0.060330	4.815319
296.269360	7999.881489	10.737421	-0.060331	4.815345
296.029992	7999.940587	10.742426	-0.060287	4.815364
296.296786	7999.891566	10.747431	-0.060336	4.815348
296.400761	8000.073928	10.752435	-0.060356	4.815401
296.439415	7999.981579	10.757440	-0.060363	4.815374
296.435619	7999.974036	10.762445	-0.060362	4.815372
296.397052	7999.885752	10.767450	-0.060355	4.815346
296.456391	7999.864291	10.772455	-0.060366	4.815340
296.352643	8000.082759	10.777459	-0.060347	4.815404
296.249714	7999.880110	10.782464	-0.060328	4.815345
296.296606	7999.896921	10.787469	-0.060336	4.815350
296.198415	7999.979736	10.792474	-0.060318	4.815375
296.278790	7999.958623	10.797479	-0.060333	4.815368
296.286618	8000.005784	10.802483	-0.060335	4.815382
296.307825	7999.860773	10.807488	-0.060339	4.815339
296.282372	8000.007855	10.812493	-0.060334	4.815382
296.397348	7999.861190	10.817498	-0.060355	4.815339
296.558364	7999.876686	10.822503	-0.060385	4.815343
296.411815	8000.003591	10.827507	-0.060358	4.815380
296.418475	7999.912850	10.832512	-0.060359	4.815354
296.479359	8000.041056	10.837517	-0.060371	4.815391
296.265727	7999.850467	10.842522	-0.060331	4.815336
296.157346	7999.992969	10.847527	-0.060311	4.815379
296.384669	8000.008494	10.852531	-0.060353	4.815382
296.618460	7999.965340	10.857536	-0.060397	4.815368
296.419734	7999.999459	10.862541	-0.060360	4.815379
296.452744	8000.000008	10.867546	-0.060366	4.815379
296.432152	7999.910953	10.872551	-0.060362	4.815353
296.398238	7999.983075	10.877555	-0.060356	4.815375
296.631007	7999.969832	10.882560	-0.060399	4.815370
296.486833	8000.001648	10.887565	-0.060372	4.815380
296.441672	7999.873707	10.892570	-0.060364	4.815342
296.619286	7999.915131	10.897575	-0.060397	4.815354
296.444863	8000.101431	10.902579	-0.060365	4.815409
296.524679	7999.850504	10.907584	-0.060379	4.815335
296.363516	7999.998544	10.912589	-0.060349	4.815379
296.597890	7999.968226	10.917594	-0.060393	4.815369
296.490097	7999.987819	10.922599	-0.060373	4.815375
296.403422	8000.029139	10.927603	-0.060357	4.815388
296.596461	7999.839944	10.932608	-0.060393	4.815332
296.683639	8000.067990	10.937613	-0.060409	4.815398
296.643613	7999.977543	10.942618	-0.060402	4.815372
296.638552	7999.964635	10.947623	-0.060401	4.815368
296.448134	7999.975376	10.952627	-0.060365	4.815372
296.524538	7999.906099	10.957632	-0.060380	4.815351
296.298668	8000.097960	10.962637	-0.060338	4.815409
296.311582	7999.964568	10.967642	-0.060340	4.815370
296.557408	7999.783730	10.972647	-0.060386	4.815316
296.521319	7999.990493	10.977651	-0.060379	4.815376
296.314640	7999.879115	10.982656	-0.060341	4.815345
296.337168	7999.985307	10.987661	-0.060345	4.815375
296.596463	7999.975710	10.992666	-0.060393	4.815371
296.588468	7999.858004	10.997671	-0.060392	4.815337
296.435957	7999.884338	11.002675	-0.060363	4.815345
296.495744	7999.869298	11.007680	-0.060374	4.815341
296.326291	7999.908177	11.012685	-0.060343	4.815353
296.417163	7999.919304	11.017690	-0.060360	4.815356
296.854084	7999.931890	11.022695	-0.060441	4.815357
296.537341	7999.941607	11.027699	-0.060382	4.815362
296.588902	7999.933912	11.032704	-0.060392	4.815359
296.648297	7999.971240	11.037709	-0.060403	4.815370
296.615917	7999.852061	11.042714	-0.060397	4.815335
296.499927	7999.982680	11.047719	-0.060375	4.815374
296.613733	8000.170551	11.052723	-0.060397	4.815428
296.708238	7999.869629	11.057728	-0.060414	4.815340
296.590722	8000.009842	11.062733	-0.060392	4.815381
296.319319	8000.037413	11.067738	-0.060342	4.815391
296.535228	8000.035648	11.072743	-0.060382	4.815389
296.432502	8000.029672	11.077747	-0.060363	4.815388
296.586276	7999.898613	11.082752	-0.060391	4.815349
296.515641	7999.990436	11.087757	-0.060378	4.815376
296.560814	7999.854372	11.092762	-0.060387	4.815336
296.456325	7999.895397	11.097767	-0.060367	4.815349
296.451160	7999.987235	11.102771	-0.060366	4.815375
296.540396	7999.866865	11.107776	-0.060383	4.815340
296.353537	7999.871253	11.112781	-0.060348	4.815342
296.322205	7999.961588	11.117786	-0.060342	4.815369
296.583988	7999.989442	11.122791	-0.060391	4.815375
296.627351	8000.168665	11.127795	-0.060399	4.815428
296.603783	8000.009013	11.132800	-0.060395	4.815381
296.752823	7999.965524	11.137805	-0.060423	4.815368
296.697753	7999.944304	11.142810	-0.060412	4.815362
296.617036	7999.930142	11.147815	-0.060397	4.815358
296.431509	7999.890729	11.152819	-0.060363	4.815347
296.470077	7999.965121	11.157824	-0.060370	4.815369
296.507721	8000.034153	11.162829	-0.060377	4.815389
296.584173	7999.950982	11.167834	-0.060391	4.815364
296.639765	7999.884566	11.172839	-0.060402	4.815345
296.725245	7999.954391	11.177843	-0.060418	4.815365
296.599997	7999.893530	11.182848	-0.060394	4.815347
296.501144	7999.985954	11.187853	-0.060376	4.815375
296.866839	7999.996291	11.192858	-0.060444	4.815376
296.860420	7999.952363	11.197863	-0.060443	4.815363
296.648535	7999.965955	11.202867	-0.060404	4.815368
296.851941	7999.868854	11.207872	-0.060441	4.815339
296.597015	7999.904180	11.212877	-0.060394	4.815350
296.528472	7999.974659	11.217882	-0.060381	4.815371
296.846695	7999.865565	11.222887	-0.060440	4.815338
296.638204	7999.889903	11.227891	-0.060402	4.815346
296.528854	7999.980015	11.232896	-0.060381	4.815373
296.628311	7999.873710	11.237901	-0.060400	4.815341
296.599030	7999.961942	11.242906	-0.060395	4.815367
296.723961	7999.912708	11.247911	-0.060418	4.815352
296.561514	7999.970943	11.252915	-0.060388	4.815370
296.716141	8000.000229	11.257920	-0.060416	4.815378
296.716095	8000.021607	11.262925	-0.060416	4.815384
296.395449	8000.016296	11.267930	-0.060357	4.815384
296.499389	8000.021226	11.272935	-0.060376	4.815385
296.644705	7999.888959	11.277939	-0.060403	4.815346
296.674393	7999.955722	11.282944	-0.060409	4.815365
296.538659	7999.986609	11.287949	-0.060383	4.815375
296.682299	7999.996473	11.292954	-0.060410	4.815377
296.711305	7999.906102	11.297959	-0.060416	4.815350
296.637077	8000.013898	11.302963	-0.060402	4.815382
296.798448	7999.868001	11.307968	-0.060432	4.815339
296.774971	7999.877234	11.312973	-0.060427	4.815342
296.693614	7999.858786	11.317978	-0.060412	4.815337
296.649610	7999.916846	11.322983	-0.060404	4.815354
296.602088	7999.864755	11.327987	-0.060395	4.815339
296.634245	7999.989277	11.332992	-0.060401	4.815375
296.510895	8000.007544	11.337997	-0.060378	4.815381
296.665279	8000.031481	11.343002	-0.060407	4.815387
296.753449	7999.916437	11.348007	-0.060424	4.815353
296.424270	8000.088416	11.353011	-0.060362	4.815405
296.457759	7999.944676	11.358016	-0.060369	4.815363
296.612293	7999.940825	11.363021	-0.060397	4.815361
296.501285	7999.958227	11.368026	-0.060377	4.815367
296.566559	7999.865250	11.373031	-0.060389	4.815339
296.642985	7999.984093	11.378035	-0.060403	4.815374
296.711230	7999.850549	11.383040	-0.060416	4.815334
296.616251	7999.988998	11.388045	-0.060398	4.815375
296.676207	7999.993200	11.393050	-0.060409	4.815376
296.777075	7999.880504	11.398055	-0.060428	4.815343
296.756831	7999.976368	11.403059	-0.060425	4.815371
296.915736	7999.794089	11.408064	-0.060454	4.815317
296.950899	7999.973175	11.413069	-0.060461	4.815369
296.506929	8000.000023	11.418074	-0.060378	4.815379
296.583531	7999.784315	11.423079	-0.060392	4.815316
296.724230	7999.983319	11.428083	-0.060419	4.815373
296.585187	7999.933986	11.433088	-0.060393	4.815359
296.747572	7999.887511	11.438093	-0.060423	4.815345
296.758829	7999.875941	11.443098	-0.060425	4.815341
296.980164	7999.910608	11.448103	-0.060466	4.815350
296.876529	7999.984782	11.453107	-0.060447	4.815373
296.847981	8000.005688	11.458112	-0.060442	4.815379
296.978515	7999.965098	11.463117	-0.060466	4.815366
296.575917	7999.975530	11.468122	-0.060391	4.815371
296.651011	7999.876303	11.473127	-0.060405	4.815342
296.516444	7999.880488	11.478131	-0.060380	4.815344
296.711437	7999.874101	11.483136	-0.060416	4.815341
296.609377	7999.894858	11.488141	-0.060397	4.815348
296.733643	7999.886230	11.493146	-0.060420	4.815345
296.733395	7999.785754	11.498151	-0.060420	4.815315
296.661147	7999.964128	11.503155	-0.060407	4.815368
296.543552	7999.969663	11.508160	-0.060385	4.815370
296.770670	7999.991599	11.513165	-0.060428	4.815375
296.759752	8000.012797	11.518170	-0.060426	4.815381
296.803309	7999.882050	11.523175	-0.060434	4.815343
296.840268	8000.019479	11.528179	-0.060441	4.815383
296.936094	7999.902424	11.533184	-0.060458	4.815348
296.870377	7999.876753	11.538189	-0.060446	4.815341
296.838184	7999.951042	11.543194	-0.060440	4.815363
296.937019	7999.909927	11.548199	-0.060459	4.815350
296.881889	7999.995594	11.553203	-0.060448	4.815376
296.843292	7999.900895	11.558208	-0.060441	4.815348
296.859066	7999.886194	11.563213	-0.060444	4.815344
296.978391	7999.971545	11.568218	-0.060466	4.815368
296.946422	7999.869474	11.573223	-0.060460	4.815339
296.782332	7999.880652	11.578227	-0.060430	4.815343
296.901957	7999.873016	11.583232	-0.060452	4.815340
296.681996	7999.896095	11.588237	-0.060411	4.815348
296.577885	7999.978812	11.593242	-0.060392	4.815372
296.801010	7999.884175	11.598247	-0.060433	4.815344
296.601494	8000.001653	11.603251	-0.060396	4.815379
296.667617	7999.957857	11.608256	-0.060409	4.815366
296.793964	8000.013396	11.613261	-0.060432	4.815381
296.794730	7999.907593	11.618266	-0.060432	4.815350
296.731583	7999.948234	11.623271	-0.060421	4.815363
296.525447	8000.070946	11.628275	-0.060382	4.815399
296.734298	7999.915147	11.633280	-0.060421	4.815353
296.690615	7999.963593	11.638285	-0.060413	4.815367
296.712807	7999.971445	11.643290	-0.060417	4.815370
296.818581	7999.796836	11.648295	-0.060437	4.815318
296.712879	7999.907317	11.653299	-0.060417	4.815351
296.642944	7999.971361	11.658304	-0.060404	4.815370
296.897939	7999.887941	11.663309	-0.060452	4.815344
296.622187	7999.975296	11.668314	-0.060400	4.815371
296.819571	7999.884508	11.673319	-0.060437	4.815344
296.728476	7999.968509	11.678323	-0.060420	4.815369
296.806489	7999.888570	11.683328	-0.060435	4.815345
296.668386	8000.012410	11.688333	-0.060409	4.815382
296.645717	7999.962868	11.693338	-0.060405	4.815367
296.934151	7999.876795	11.698343	-0.060459	4.815341
296.985503	7999.973846	11.703347	-0.060468	4.815369
296.833148	7999.865505	11.708352	-0.060440	4.815338
296.679301	8000.108798	11.713357	-0.060411	4.815410
296.794506	8000.128880	11.718362	-0.060433	4.815415
296.917121	8000.000511	11.723367	-0.060456	4.815377
296.804740	7999.991168	11.728371	-0.060435	4.815375
296.801576	7999.862853	11.733376	-0.060434	4.815337
296.940575	7999.985940	11.738381	-0.060460	4.815373
296.899823	7999.998093	11.743386	-0.060452	4.815376
297.117896	7999.894821	11.748391	-0.060493	4.815345
296.951388	7999.960471	11.753395	-0.060462	4.815365
296.828269	7999.845133	11.758400	-0.060439	4.815332
296.787408	7999.828424	11.763405	-0.060431	4.815327
296.946583	7999.980705	11.768410	-0.060461	4.815371
296.985596	7999.897981	11.773415	-0.060468	4.815347
296.746976	7999.997709	11.778419	-0.060424	4.815377
296.814746	7999.940046	11.783424	-0.060437	4.815360
296.793376	7999.901215	11.788429	-0.060433	4.815349
296.637358	7999.971314	11.793434	-0.060404	4.815370
296.895777	7999.785340	11.798439	-0.060452	4.815314
296.814596	7999.986012	11.803443	-0.060437	4.815373
296.645472	7999.983211	11.808448	-0.060405	4.815373
296.549067	7999.930310	11.813453	-0.060387	4.815358
296.721168	8000.079599	11.818458	-0.060420	4.815401
296.847888	7999.968400	11.823463	-0.060443	4.815368
296.561548	8000.094058	11.828467	-0.060390	4.815406
296.893869	7999.909308	11.833472	-0.060452	4.815350
296.956164	8000.113429	11.838477	-0.060463	4.815410
296.920018	7999.962120	11.843482	-0.060457	4.815366
297.002126	7999.887592	11.848487	-0.060472	4.815344
296.968885	8000.104025	11.853491	-0.060466	4.815407
296.926737	7999.953685	11.858496	-0.060458	4.815363
297.052937	7999.991051	11.863501	-0.060481	4.815374
297.075989	8000.067326	11.868506	-0.060486	4.815396
297.031030	7999.889148	11.873511	-0.060477	4.815344
296.734298	8000.094801	11.878515	-0.060422	4.815405
296.849570	7999.871181	11.883520	-0.060444	4.815340
296.895384	7999.926454	11.888525	-0.060452	4.815355
296.835355	8000.012039	11.893530	-0.060441	4.815381
296.999289	7999.792433	11.898535	-0.060471	4.815316
296.946427	8000.060914	11.903539	-0.060462	4.815395
296.869478	7999.995508	11.908544	-0.060447	4.815376
297.065343	7999.889731	11.913549	-0.060484	4.815344
296.916204	7999.873366	11.918554	-0.060456	4.815340
297.127139	7999.877932	11.923559	-0.060495	4.815340
296.960108	8000.025877	11.928563	-0.060464	4.815384
296.928262	7999.791268	11.933568	-0.060458	4.815316
296.951861	7999.891065	11.938573	-0.060463	4.815345
296.689970	7999.895278	11.943578	-0.060414	4.815347
297.080822	7999.971234	11.948583	-0.060487	4.815368
297.081116	7999.887868	11.953587	-0.060487	4.815343
296.796203	7999.965451	11.958592	-0.060434	4.815367
296.845246	7999.831588	11.963597	-0.060443	4.815328
297.008152	7999.973242	11.968602	-0.060473	4.815369
297.069657	7999.983883	11.973607	-0.060485	4.815371
296.966036	7999.889176	11.978611	-0.060466	4.815344
296.855473	7999.876657	11.983616	-0.060445	4.815341
296.921870	7999.986784	11.988621	-0.060457	4.815373
296.985085	7999.957904	11.993626	-0.060469	4.815364
297.042133	7999.864791	11.998631	-0.060480	4.815337
296.983972	8000.000644	12.003635	-0.060469	4.815377
297.063205	7999.879039	12.008640	-0.060484	4.815341
297.054027	7999.897059	12.013645	-0.060482	4.815346
296.772706	7999.981115	12.018650	-0.060430	4.815372
296.957913	7999.866610	12.023655	-0.060464	4.815338
297.187549	7999.902483	12.028659	-0.060507	4.815347
296.897913	7999.982126	12.033664	-0.060453	4.815372
297.146459	7999.877222	12.038669	-0.060499	4.815340
297.068280	7999.961438	12.043674	-0.060485	4.815365
296.938773	7999.792550	12.048679	-0.060461	4.815316
296.915853	7999.881956	12.053683	-0.060457	4.815342
297.043060	7999.886204	12.058688	-0.060480	4.815343
297.065880	7999.789316	12.063693	-0.060484	4.815315
296.857326	7999.973983	12.068698	-0.060446	4.815370
296.964021	7999.880624	12.073703	-0.060466	4.815342
296.902809	8000.019633	12.078707	-0.060454	4.815383
296.770948	7999.894530	12.083712	-0.060430	4.815347
296.890094	8000.023701	12.088717	-0.060452	4.815384
296.846767	7999.978092	12.093722	-0.060444	4.815371
296.742795	7999.796802	12.098727	-0.060424	4.815318
297.008070	7999.994664	12.103731	-0.060474	4.815375
297.021168	8000.003434	12.108736	-0.060476	4.815377
297.097332	8000.010043	12.113741	-0.060491	4.815379
296.983562	7999.985712	12.118746	-0.060469	4.815372
297.173095	7999.959996	12.123751	-0.060505	4.815364
296.961438	7999.960765	12.128755	-0.060465	4.815365
297.055873	7999.971952	12.133760	-0.060483	4.815368
297.147351	7999.892235	12.138765	-0.060500	4.815344
297.135723	8000.034205	12.143770	-0.060498	4.815386
297.206359	7999.980864	12.148775	-0.060511	4.815370
297.164900	8000.052863	12.153779	-0.060503	4.815391
297.068008	7999.877031	12.158784	-0.060485	4.815340
297.168730	7999.858393	12.163789	-0.060504	4.815334
297.196924	7999.977508	12.168794	-0.060509	4.815369
297.084591	7999.984199	12.173799	-0.060488	4.815371
296.921567	7999.997532	12.178803	-0.060458	4.815376
296.856142	7999.858565	12.183808	-0.060446	4.815336
297.002457	7999.979636	12.188813	-0.060473	4.815370
297.137411	7999.896364	12.193818	-0.060498	4.815345
297.136864	7999.971178	12.198823	-0.060498	4.815367
297.086744	7999.994933	12.203827	-0.060489	4.815375
296.994755	7999.773223	12.208832	-0.060472	4.815310
297.006363	7999.900612	12.213837	-0.060474	4.815347
296.950020	7999.980915	12.218842	-0.060464	4.815371
297.177433	7999.881004	12.223847	-0.060506	4.815341
297.267534	8000.000076	12.228851	-0.060523	4.815375
297.119592	8000.045725	12.233856	-0.060495	4.815389
297.167034	7999.897939	12.238861	-0.060504	4.815346
297.065236	7999.963593	12.243866	-0.060485	4.815365
297.030310	7999.965153	12.248871	-0.060479	4.815366
296.932401	8000.057594	12.253875	-0.060460	4.815394
297.034354	7999.979119	12.258880	-0.060479	4.815370
296.930568	7999.871583	12.263885	-0.060460	4.815339
296.773218	7999.992966	12.268890	-0.060431	4.815375
296.871732	7999.886644	12.273895	-0.060449	4.815344
296.903556	7999.889311	12.278899	-0.060455	4.815345
296.726742	7999.980443	12.283904	-0.060422	4.815372
297.065791	7999.924069	12.288909	-0.060485	4.815354
297.113165	8000.132219	12.293914	-0.060494	4.815414
297.065112	7999.917648	12.298919	-0.060485	4.815352
297.020045	8000.099681	12.303923	-0.060477	4.815405
296.937396	8000.001045	12.308928	-0.060462	4.815377
297.164828	7999.895790	12.313933	-0.060504	4.815345
296.894944	7999.998207	12.318938	-0.060454	4.815376
296.890557	7999.979965	12.323943	-0.060453	4.815371
297.074087	8000.007592	12.328947	-0.060487	4.815378
296.944090	7999.933825	12.333952	-0.060463	4.815357
297.059935	7999.988121	12.338957	-0.060485	4.815373
296.925922	8000.103479	12.343962	-0.060460	4.815407
296.908627	7999.888350	12.348967	-0.060456	4.815344
296.974062	8000.078627	12.353971	-0.060469	4.815399
296.937749	8000.027789	12.358976	-0.060462	4.815385
297.068743	7999.990414	12.363981	-0.060486	4.815373
296.873374	8000.060930	12.368986	-0.060450	4.815395
297.073449	7999.890021	12.373991	-0.060487	4.815344
297.180117	7999.923856	12.378995	-0.060507	4.815353
297.093760	7999.979077	12.384000	-0.060491	4.815370
297.090050	7999.946951	12.389005	-0.060490	4.815360
297.121602	7999.997713	12.394010	-0.060496	4.815375
297.147337	7999.876289	12.399015	-0.060501	4.815340
296.904185	8000.020835	12.404019	-0.060456	4.815383
297.117736	7999.981621	12.409024	-0.060496	4.815370
297.161106	7999.994099	12.414029	-0.060504	4.815374
297.066407	8000.029942	12.419034	-0.060486	4.815385
297.207771	7999.889057	12.424039	-0.060512	4.815343
297.072284	8000.126243	12.429043	-0.060487	4.815413
296.822478	8000.098588	12.434048	-0.060441	4.815406
296.957435	7999.864605	12.439053	-0.060466	4.815337
297.070073	8000.101627	12.444058	-0.060487	4.815406
297.044208	7999.999656	12.449063	-0.060482	4.815376
296.928002	7999.907946	12.454067	-0.060460	4.815350
296.891786	7999.971480	12.459072	-0.060454	4.815369
297.176259	7999.886410	12.464077	-0.060507	4.815342
296.912146	7999.971821	12.469082	-0.060457	4.815369
296.925441	7999.841640	12.474087	-0.060460	4.815331
297.144150	8000.028044	12.479091	-0.060501	4.815384
297.167782	7999.976063	12.484096	-0.060505	4.815369
297.159585	7999.788875	12.489101	-0.060504	4.815314
296.989518	7999.988076	12.494106	-0.060472	4.815373
296.972201	7999.958931	12.499111	-0.060469	4.815365
296.880886	8000.008725	12.504115	-0.060452	4.815380
296.946938	7999.858041	12.509120	-0.060464	4.815335
297.323486	7999.956207	12.514125	-0.060534	4.815362
297.086191	7999.969378	12.519130	-0.060490	4.815367
297.174910	7999.876789	12.524135	-0.060507	4.815340
297.134832	7999.980876	12.529139	-0.060499	4.815370
297.108380	8000.151461	12.534144	-0.060494	4.815420
297.293762	7999.859523	12.539149	-0.060529	4.815334
297.181553	7999.980587	12.544154	-0.060508	4.815370
297.250524	7999.991351	12.549159	-0.060521	4.815373
297.350236	7999.984455	12.554163	-0.060539	4.815370
297.425584	7999.939743	12.559168	-0.060553	4.815357
297.421249	7999.914020	12.564173	-0.060553	4.815349
297.192501	7999.962606	12.569178	-0.060510	4.815365
297.238349	7999.978332	12.574183	-0.060519	4.815369
297.255241	7999.913411	12.579187	-0.060522	4.815350
297.296799	7999.979304	12.584192	-0.060530	4.815369
297.258285	7999.891019	12.589197	-0.060522	4.815343
296.829150	8000.110510	12.594202	-0.060443	4.815409
296.984833	7999.973069	12.599207	-0.060472	4.815369
296.892129	7999.948019	12.604211	-0.060454	4.815362
296.990156	7999.973161	12.609216	-0.060473	4.815369
297.219946	7999.905356	12.614221	-0.060515	4.815348
297.135719	7999.965957	12.619226	-0.060500	4.815366
297.214342	7999.958711	12.624231	-0.060514	4.815363
297.336530	8000.056938	12.629235	-0.060537	4.815391
297.280198	7999.976908	12.634240	-0.060527	4.815368
297.090214	7999.975898	12.639245	-0.060491	4.815369
297.042221	8000.110853	12.644250	-0.060482	4.815409
297.383231	7999.965794	12.649255	-0.060546	4.815365
297.329897	8000.009805	12.654259	-0.060536	4.815378
297.141099	8000.066535	12.659264	-0.060501	4.815395
297.188705	8000.013881	12.664269	-0.060510	4.815380
297.129735	8000.021456	12.669274	-0.060499	4.815382
297.177554	7999.892916	12.674279	-0.060508	4.815344
297.199978	8000.133789	12.679283	-0.060512	4.815414
297.118613	7999.975315	12.684288	-0.060497	4.815369
297.194152	7999.861130	12.689293	-0.060511	4.815335
297.282188	8000.009028	12.694298	-0.060527	4.815378
297.225583	7999.962129	12.699303	-0.060517	4.815364
297.270161	7999.966076	12.704307	-0.060525	4.815365
297.071248	7999.986296	12.709312	-0.060488	4.815372
297.209663	7999.872084	12.714317	-0.060514	4.815338
297.161808	7999.885188	12.719322	-0.060505	4.815342
296.927402	7999.986055	12.724327	-0.060461	4.815373
297.173658	7999.981587	12.729331	-0.060507	4.815370
297.337368	7999.871001	12.734336	-0.060538	4.815337
297.393967	7999.898663	12.739341	-0.060548	4.815345
297.219017	7999.973793	12.744346	-0.060516	4.815368
297.282011	7999.865813	12.749351	-0.060527	4.815336
297.373587	7999.945361	12.754355	-0.060544	4.815359
297.050317	7999.971002	12.759360	-0.060484	4.815368
297.151544	7999.785628	12.764365	-0.060503	4.815313
297.263890	7999.978821	12.769370	-0.060524	4.815369
297.122007	7999.940129	12.774375	-0.060498	4.815358
297.165100	7999.934432	12.779379	-0.060506	4.815356
297.124778	7999.928421	12.784384	-0.060498	4.815355
297.325598	7999.844103	12.789389	-0.060536	4.815329
297.202068	7999.995976	12.794394	-0.060513	4.815374
297.328425	7999.973487	12.799399	-0.060536	4.815367
297.116144	7999.868427	12.804403	-0.060497	4.815337
297.160741	7999.979262	12.809408	-0.060505	4.815370
297.470379	7999.905299	12.814413	-0.060563	4.815346
297.358966	7999.940865	12.819418	-0.060542	4.815357
297.233539	7999.893895	12.824423	-0.060519	4.815344
297.267294	7999.906214	12.829427	-0.060525	4.815348
297.334851	7999.887026	12.834432	-0.060538	4.815342
297.189102	7999.987225	12.839437	-0.060510	4.815372
297.209699	8000.008946	12.844442	-0.060514	4.815378
297.265512	7999.961773	12.849447	-0.060525	4.815364
297.264033	7999.995954	12.854451	-0.060524	4.815374
297.251274	7999.862134	12.859456	-0.060522	4.815335
297.200103	7999.894423	12.864461	-0.060513	4.815345
297.219959	8000.000573	12.869466	-0.060516	4.815375
297.210748	7999.856123	12.874471	-0.060515	4.815333
297.245192	7999.993513	12.879475	-0.060521	4.815373
297.412585	7999.968498	12.884480	-0.060552	4.815365
297.408014	7999.875431	12.889485	-0.060551	4.815338
297.334947	7999.988592	12.894490	-0.060538	4.815371
297.353362	7999.877735	12.899495	-0.060541	4.815339
297.409175	8000.002653	12.904499	-0.060552	4.815375
297.211545	7999.963036	12.909504	-0.060515	4.815365
297.195171	7999.941389	12.914509	-0.060512	4.815358
297.376950	8000.005330	12.919514	-0.060546	4.815376
297.233978	7999.903556	12.924519	-0.060519	4.815347
297.099890	7999.868200	12.929523	-0.060494	4.815337
297.318516	8000.010780	12.934528	-0.060535	4.815378
297.449177	7999.888957	12.939533	-0.060559	4.815342
297.126177	7999.987286	12.944538	-0.060499	4.815372
297.303663	7999.877997	12.949543	-0.060532	4.815339
297.453691	7999.911483	12.954547	-0.060560	4.815348
297.349809	7999.966414	12.959552	-0.060541	4.815365
297.417837	7999.864930	12.964557	-0.060553	4.815335
297.256887	8000.064283	12.969562	-0.060524	4.815394
297.340899	7999.961996	12.974567	-0.060539	4.815364
297.269451	7999.926609	12.979571	-0.060526	4.815354
297.360731	7999.970879	12.984576	-0.060543	4.815366
297.255033	7999.893238	12.989581	-0.060523	4.815344
297.241163	8000.002036	12.994586	-0.060521	4.815376
297.111013	8000.099287	12.999591	-0.060497	4.815405
297.293300	7999.958010	13.004595	-0.060530	4.815363
297.129726	8000.046156	13.009600	-0.060500	4.815389
297.402366	7999.898895	13.014605	-0.060551	4.815345
297.390772	8000.046211	13.019610	-0.060549	4.815388
297.444444	7999.892114	13.024615	-0.060559	4.815343
297.206486	7999.989715	13.029619	-0.060514	4.815372
297.194356	7999.960656	13.034624	-0.060512	4.815364
297.346438	7999.773987	13.039629	-0.060540	4.815309
297.164995	8000.124781	13.044634	-0.060507	4.815412
297.259010	7999.941424	13.049639	-0.060524	4.815358
297.440130	7999.998941	13.054643	-0.060558	4.815374
297.198456	8000.125341	13.059648	-0.060513	4.815412
297.289436	7999.925900	13.064653	-0.060530	4.815353
297.232341	7999.929231	13.069658	-0.060519	4.815355
297.177948	7999.976431	13.074663	-0.060509	4.815369
297.117287	8000.018182	13.079667	-0.060498	4.815381
297.051913	7999.939072	13.084672	-0.060486	4.815358
297.423181	8000.004016	13.089677	-0.060555	4.815375
297.155164	8000.171666	13.094682	-0.060505	4.815426
297.131174	7999.938253	13.099687	-0.060501	4.815358
297.305464	7999.911215	13.104691	-0.060533	4.815349
297.351973	7999.902367	13.109696	-0.060542	4.815346
297.314096	7999.931670	13.114701	-0.060535	4.815355
297.222567	8000.004977	13.119706	-0.060518	4.815377
297.193502	7999.971361	13.124711	-0.060512	4.815367
297.132421	7999.885909	13.129715	-0.060501	4.815342
297.138255	7999.993964	13.134720	-0.060502	4.815374
297.253041	7999.969146	13.139725	-0.060523	4.815366
297.124320	8000.002288	13.144730	-0.060500	4.815376
297.097631	7999.933439	13.149735	-0.060495	4.815356
297.340082	7999.946010	13.154739	-0.060540	4.815359
297.262677	7999.981071	13.159744	-0.060525	4.815370
297.203336	7999.937333	13.164749	-0.060514	4.815357
297.112051	8000.128221	13.169754	-0.060497	4.815413
297.242771	7999.862100	13.174759	-0.060522	4.815335
297.142369	7999.985497	13.179763	-0.060503	4.815371
297.051899	7999.920935	13.184768	-0.060486	4.815353
297.309278	7999.949787	13.189773	-0.060534	4.815360
297.205369	7999.997235	13.194778	-0.060515	4.815375
297.244600	7999.979716	13.199783	-0.060522	4.815369
297.415855	7999.876736	13.204787	-0.060554	4.815338
297.312586	7999.980846	13.209792	-0.060535	4.815369
297.451510	8000.013079	13.214797	-0.060561	4.815378
297.392828	7999.878498	13.219802	-0.060550	4.815339
297.231552	7999.953855	13.224807	-0.060520	4.815362
297.332738	8000.012184	13.229811	-0.060539	4.815378
297.140535	8000.046411	13.234816	-0.060503	4.815389
297.409601	7999.992084	13.239821	-0.060553	4.815372
297.267108	7999.985448	13.244826	-0.060527	4.815371
297.151703	7999.844583	13.249831	-0.060505	4.815330
297.431465	8000.020243	13.254835	-0.060557	4.815380
297.324951	7999.966103	13.259840	-0.060537	4.815365
297.384507	7999.875168	13.264845	-0.060548	4.815338
297.234825	8000.111050	13.269850	-0.060521	4.815408
297.328458	7999.894551	13.274855	-0.060538	4.815344
297.344763	7999.974990	13.279859	-0.060541	4.815367
297.317828	7999.976683	13.284864	-0.060536	4.815368
297.429014	7999.984941	13.289869	-0.060557	4.815370
297.235972	7999.996707	13.294874	-0.060521	4.815374
297.276149	7999.993099	13.299879	-0.060528	4.815373
297.549093	7999.998694	13.304883	-0.060579	4.815373
297.271877	7999.995169	13.309888	-0.060528	4.815374
297.136132	7999.864656	13.314893	-0.060502	4.815336
297.137800	8000.032499	13.319898	-0.060503	4.815385
297.474461	7999.917297	13.324903	-0.060565	4.815350
297.405099	7999.974938	13.329907	-0.060553	4.815367
297.201736	8000.008980	13.334912	-0.060515	4.815378
297.468407	7999.927891	13.339917	-0.060564	4.815353
297.388090	8000.091170	13.344922	-0.060550	4.815401
297.295805	7999.983822	13.349927	-0.060532	4.815370
297.279757	8000.033795	13.354931	-0.060529	4.815385
297.242642	8000.002184	13.359936	-0.060522	4.815376
297.339581	7999.964244	13.364941	-0.060540	4.815364
296.953888	7999.980299	13.369946	-0.060469	4.815371
297.224709	7999.963412	13.374951	-0.060519	4.815365
297.263008	7999.987564	13.379955	-0.060526	4.815371
297.205617	8000.060367	13.384960	-0.060516	4.815393
297.489930	7999.991329	13.389965	-0.060569	4.815371
297.469585	8000.071160	13.394970	-0.060565	4.815395
297.329933	8000.098776	13.399975	-0.060539	4.815404
297.355863	7999.966665	13.404979	-0.060544	4.815365
297.206480	8000.146970	13.409984	-0.060516	4.815418
297.361818	7999.973180	13.414989	-0.060545	4.815367
297.218846	8000.013567	13.419994	-0.060518	4.815379
297.252905	7999.976723	13.424999	-0.060525	4.815368
297.245412	8000.022562	13.430003	-0.060523	4.815382
297.024699	7999.953704	13.435008	-0.060482	4.815363
297.225691	7999.954899	13.440013	-0.060520	4.815362
297.249892	8000.017297	13.445018	-0.060524	4.815380
297.121141	8000.044025	13.450023	-0.060500	4.815389
297.173025	8000.041680	13.455027	-0.060510	4.815388
297.289951	8000.056446	13.460032	-0.060532	4.815391
297.434811	7999.882483	13.465037	-0.060559	4.815340
297.236496	8000.030979	13.470042	-0.060522	4.815384
297.364639	8000.029898	13.475047	-0.060546	4.815383
297.444261	7999.991671	13.480051	-0.060560	4.815372
297.653876	7999.976976	13.485056	-0.060599	4.815366
297.505563	8000.105994	13.490061	-0.060572	4.815405
297.777365	7999.981165	13.495066	-0.060622	4.815367
297.484398	7999.942105	13.500071	-0.060568	4.815357
297.501159	7999.922076	13.505075	-0.060571	4.815351
297.739661	7999.887551	13.510080	-0.060615	4.815340
297.716345	7999.985505	13.515085	-0.060611	4.815369
297.460884	7999.979133	13.520090	-0.060564	4.815368
297.685928	8000.047000	13.525095	-0.060606	4.815387
297.766654	7999.888005	13.530099	-0.060621	4.815340
297.437977	7999.976621	13.535104	-0.060559	4.815367
297.358618	7999.933621	13.540109	-0.060545	4.815355
297.600635	7999.987872	13.545114	-0.060590	4.815370
297.444302	7999.945733	13.550119	-0.060561	4.815358
297.529010	7999.996308	13.555123	-0.060576	4.815373
297.608273	8000.053206	13.560128	-0.060591	4.815389
297.625633	7999.966915	13.565133	-0.060594	4.815364
297.424179	8000.002058	13.570138	-0.060557	4.815375
297.684555	7999.997825	13.575143	-0.060606	4.815372
297.695392	7999.859050	13.580147	-0.060607	4.815332
297.512923	8000.031325	13.585152	-0.060574	4.815383
297.493951	7999.928399	13.590157	-0.060570	4.815353
297.578113	7999.962931	13.595162	-0.060586	4.815363
297.346611	7999.975129	13.600167	-0.060543	4.815367
297.453160	7999.953381	13.605171	-0.060563	4.815360
297.447010	7999.944730	13.610176	-0.060561	4.815358
297.668540	7999.856479	13.615181	-0.060603	4.815331
297.458250	7999.990881	13.620186	-0.060564	4.815371
297.345378	8000.009321	13.625191	-0.060543	4.815377
297.510185	7999.997090	13.630195	-0.060573	4.815373
297.310452	8000.011952	13.635200	-0.060536	4.815378
297.470094	7999.978258	13.640205	-0.060566	4.815368
297.491477	8000.014956	13.645210	-0.060570	4.815378
297.447889	8000.111505	13.650215	-0.060562	4.815407
297.353295	8000.005187	13.655219	-0.060544	4.815376
297.358001	8000.000991	13.660224	-0.060545	4.815375
297.510391	7999.891286	13.665229	-0.060573	4.815342
297.375364	7999.884774	13.670234	-0.060548	4.815341
297.297637	7999.892038	13.675239	-0.060534	4.815343
297.423526	7999.890920	13.680243	-0.060557	4.815342
297.267969	7999.874448	13.685248	-0.060528	4.815338
297.418764	7999.988113	13.690253	-0.060556	4.815371
297.505310	7999.932898	13.695258	-0.060573	4.815354
297.447212	7999.983243	13.700263	-0.060562	4.815369
297.652440	7999.986647	13.705267	-0.060600	4.815369
297.583590	7999.995128	13.710272	-0.060587	4.815372
297.690749	7999.948806	13.715277	-0.060607	4.815358
297.434902	8000.000148	13.720282	-0.060560	4.815374
297.449635	7999.856095	13.725287	-0.060562	4.815332
297.706120	8000.028164	13.730291	-0.060610	4.815381
297.459704	8000.012322	13.735296	-0.060564	4.815378
297.377557	7999.875214	13.740301	-0.060549	4.815338
297.334189	8000.148132	13.745306	-0.060541	4.815418
297.389822	7999.897867	13.750311	-0.060551	4.815345
297.308727	7999.879423	13.755315	-0.060536	4.815340
297.429216	7999.864319	13.760320	-0.060559	4.815335
297.530204	7999.889510	13.765325	-0.060577	4.815341
297.379137	7999.974656	13.770330	-0.060549	4.815367
297.331735	7999.783612	13.775335	-0.060540	4.815311
297.630426	7999.910416	13.780339	-0.060596	4.815347
297.393662	7999.906494	13.785344	-0.060552	4.815347
297.450725	7999.883926	13.790349	-0.060563	4.815340
297.548393	8000.019157	13.795354	-0.060581	4.815379
297.490954	7999.963693	13.800359	-0.060570	4.815363
297.491492	7999.900640	13.805363	-0.060570	4.815345
297.506749	7999.996025	13.810368	-0.060573	4.815373
297.514588	7999.950195	13.815373	-0.060575	4.815359
297.376818	7999.904088	13.820378	-0.060549	4.815346
297.377109	8000.091151	13.825383	-0.060549	4.815401
297.503196	7999.801436	13.830387	-0.060573	4.815316
297.569724	7999.978907	13.835392	-0.060585	4.815367
297.508856	7999.907353	13.840397	-0.060574	4.815347
297.399357	7999.980361	13.845402	-0.060553	4.815369
297.394887	8000.067938	13.850407	-0.060553	4.815394
297.495642	7999.807733	13.855411	-0.060571	4.815318
297.450119	7999.970519	13.860416	-0.060563	4.815365
297.603762	7999.884350	13.865421	-0.060592	4.815340
297.531993	7999.888506	13.870426	-0.060578	4.815341
297.608423	7999.976355	13.875431	-0.060592	4.815366
297.650296	7999.795340	13.880435	-0.060600	4.815313
297.479585	7999.894056	13.885440	-0.060568	4.815343
297.524474	7999.966417	13.890445	-0.060577	4.815364
297.768186	8000.045282	13.895450	-0.060622	4.815386
297.559617	7999.949901	13.900455	-0.060583	4.815359
297.509048	7999.892413	13.905459	-0.060574	4.815342
297.425480	7999.966921	13.910464	-0.060559	4.815365
297.493145	7999.976595	13.915469	-0.060571	4.815367
297.713332	8000.002694	13.920474	-0.060612	4.815374
297.540679	7999.870498	13.925479	-0.060580	4.815336
297.605649	7999.886541	13.930483	-0.060592	4.815340
297.780718	8000.101087	13.935488	-0.060625	4.815402
297.816255	7999.993718	13.940493	-0.060631	4.815370
297.482241	7999.893052	13.945498	-0.060569	4.815343
297.467019	7999.983656	13.950503	-0.060566	4.815369
297.602647	7999.992320	13.955507	-0.060592	4.815371
297.591620	8000.014585	13.960512	-0.060590	4.815378
297.568869	7999.936181	13.965517	-0.060585	4.815355
297.472767	8000.036134	13.970522	-0.060568	4.815385
297.394262	8000.026283	13.975527	-0.060553	4.815382
297.627008	7999.877292	13.980531	-0.060596	4.815337
297.565149	7999.999191	13.985536	-0.060585	4.815373
297.565862	7999.900866	13.990541	-0.060585	4.815345
297.471096	7999.881126	13.995546	-0.060567	4.815339
297.536150	7999.985888	14.000551	-0.060579	4.815370
297.465297	7999.892791	14.005555	-0.060566	4.815343
297.429126	7999.928535	14.010560	-0.060560	4.815353
297.519021	7999.949267	14.015565	-0.060576	4.815359
297.532904	7999.965532	14.020570	-0.060579	4.815364
297.570230	7999.900950	14.025575	-0.060586	4.815345
297.739037	7999.860995	14.030579	-0.060617	4.815332
297.629508	8000.129611	14.035584	-0.060597	4.815411
297.725188	7999.964451	14.040589	-0.060615	4.815362
297.573845	8000.091280	14.045594	-0.060587	4.815400
297.597189	8000.136563	14.050599	-0.060591	4.815413
297.824924	7999.982143	14.055603	-0.060633	4.815367
297.606565	7999.974249	14.060608	-0.060593	4.815366
297.642828	7999.898961	14.065613	-0.060600	4.815344
297.683780	7999.891090	14.070618	-0.060607	4.815341
297.467112	7999.976218	14.075623	-0.060567	4.815367
297.495954	8000.007696	14.080627	-0.060572	4.815376
297.512221	8000.136235	14.085632	-0.060575	4.815414
297.517703	7999.993095	14.090637	-0.060576	4.815372
297.616097	8000.108031	14.095642	-0.060595	4.815405
297.695180	8000.059106	14.100647	-0.060610	4.815390
297.790929	8000.001905	14.105651	-0.060627	4.815373
297.726644	8000.128041	14.110656	-0.060615	4.815410
297.646260	7999.973857	14.115661	-0.060600	4.815365
297.706583	7999.888278	14.120666	-0.060612	4.815340
297.798035	8000.025546	14.125671	-0.060629	4.815380
297.675571	8000.037413	14.130675	-0.060606	4.815384
297.560065	8000.060084	14.135680	-0.060585	4.815391
297.933323	8000.027794	14.140685	-0.060654	4.815380
297.613762	8000.064184	14.145690	-0.060595	4.815392
297.710716	8000.119239	14.150695	-0.060613	4.815408
297.939289	7999.964833	14.155699	-0.060655	4.815361
297.779675	8000.014564	14.160704	-0.060625	4.815377
297.666675	7999.972074	14.165709	-0.060604	4.815365
297.723776	8000.080982	14.170714	-0.060615	4.815396
297.800730	8000.049123	14.175719	-0.060629	4.815387
297.578438	7999.900070	14.180723	-0.060588	4.815344
297.615419	8000.031090	14.185728	-0.060595	4.815382
297.801138	7999.882387	14.190733	-0.060629	4.815338
297.686564	7999.870870	14.195738	-0.060608	4.815335
297.875528	8000.037545	14.200743	-0.060643	4.815383
297.714491	7999.909816	14.205747	-0.060613	4.815346
297.539608	8000.100388	14.210752	-0.060581	4.815403
297.546388	7999.893137	14.215757	-0.060582	4.815342
297.639000	8000.020803	14.220762	-0.060600	4.815379
297.546696	8000.075926	14.225767	-0.060582	4.815396
297.562421	7999.917993	14.230771	-0.060585	4.815350
297.514382	8000.005916	14.235776	-0.060576	4.815375
297.617241	7999.983038	14.240781	-0.060596	4.815368
297.695202	8000.022813	14.245786	-0.060610	4.815380
297.480960	8000.088741	14.250791	-0.060570	4.815400
297.675698	7999.848263	14.255795	-0.060606	4.815329
297.639331	7999.468212	14.260800	-0.060599	4.815218
297.489056	7996.363124	14.265805	-0.060569	4.814311
297.681863	7990.783502	14.270810	-0.060602	4.812680
297.609662	7983.942383	14.275815	-0.060584	4.810681
297.580833	7976.677876	14.280819	-0.060574	4.808557
297.503856	7969.045623	14.285824	-0.060554	4.806324
297.675173	7961.215025	14.290829	-0.060581	4.804031
297.535995	7953.344943	14.295834	-0.060550	4.801727
297.362210	7945.332219	14.300839	-0.060513	4.799381
297.459915	7937.455356	14.305843	-0.060526	4.797071
297.271813	7929.416235	14.310848	-0.060485	4.794714
297.389788	7921.406913	14.315853	-0.060502	4.792364
297.413502	7913.396931	14.320858	-0.060501	4.790012
297.445546	7905.395251	14.325863	-0.060502	4.787662
297.333644	7897.366789	14.330867	-0.060476	4.785303
297.173538	7889.383071	14.335872	-0.060441	4.782957
297.505193	7881.386737	14.340877	-0.060498	4.780604
297.366071	7873.455740	14.345882	-0.060467	4.778270
297.102408	7865.388147	14.350887	-0.060412	4.775896
297.274055	7857.396082	14.355891	-0.060439	4.773541
297.140488	7849.314997	14.360896	-0.060409	4.771160
297.022869	7841.355705	14.365901	-0.060382	4.768813
296.991483	7833.369725	14.370906	-0.060371	4.766457
297.123376	7825.328398	14.375911	-0.060390	4.764083
296.873646	7817.434370	14.380915	-0.060339	4.761753
296.913439	7809.321700	14.385920	-0.060341	4.759356
297.162519	7801.377124	14.390925	-0.060382	4.757007
296.976258	7793.365914	14.395930	-0.060342	4.754638
296.720828	7785.311576	14.400935	-0.060289	4.752256
296.889938	7777.288274	14.405939	-0.060316	4.749880
296.842546	7769.331883	14.410944	-0.060302	4.747523
296.682920	7761.323489	14.415949	-0.060267	4.745151
296.544505	7753.362556	14.420954	-0.060236	4.742791
296.586298	7745.329662	14.425959	-0.060238	4.740408
296.756461	7737.319989	14.430963	-0.060265	4.738030
296.563281	7729.302229	14.435968	-0.060224	4.735650
296.719936	7721.319338	14.440973	-0.060248	4.733278
296.556202	7713.294256	14.445978	-0.060212	4.730893
296.426482	7705.296704	14.450983	-0.060183	4.728515
296.457846	7697.272204	14.455987	-0.060183	4.726127
296.575160	7689.309151	14.460992	-0.060200	4.723756
296.405770	7681.298266	14.465997	-0.060163	4.721371
296.427964	7673.303638	14.471002	-0.060162	4.718988
296.398643	7665.356580	14.476007	-0.060151	4.716619
296.538022	7657.346919	14.481011	-0.060172	4.714229
296.148036	7649.248098	14.486016	-0.060094	4.711813
296.116018	7641.263034	14.491021	-0.060083	4.709429
296.091469	7633.292539	14.496026	-0.060073	4.707048
296.056720	7625.257101	14.501031	-0.060062	4.704646
296.113814	7617.373619	14.506035	-0.060067	4.702288
296.128330	7609.229856	14.511040	-0.060065	4.699852
296.199962	7601.354497	14.516045	-0.060073	4.697494
296.057122	7593.325315	14.521050	-0.060041	4.695089
296.019126	7585.252042	14.526055	-0.060029	4.692670
295.835459	7577.263231	14.531059	-0.059989	4.690275
295.926350	7569.282348	14.536064	-0.060001	4.687881
295.969208	7561.214755	14.541069	-0.060004	4.685460
295.836085	7553.306222	14.546074	-0.059974	4.683085
295.799521	7545.295292	14.551079	-0.059962	4.680678
295.948901	7537.354921	14.556083	-0.059985	4.678291
295.832878	7529.298868	14.561088	-0.059958	4.675868
295.730380	7521.203546	14.566093	-0.059933	4.673433
295.807969	7513.168302	14.571098	-0.059943	4.671013
295.670922	7505.138285	14.576103	-0.059912	4.668595
295.761898	7497.237773	14.581107	-0.059924	4.666214
295.569392	7489.192051	14.586112	-0.059883	4.663788
295.621494	7481.222967	14.591117	-0.059887	4.661384
295.700001	7473.239470	14.596122	-0.059897	4.658974
295.458696	7465.228950	14.601127	-0.059846	4.656555
295.539265	7457.240327	14.606131	-0.059856	4.654141
295.411407	7449.197336	14.611136	-0.059827	4.651709
295.338407	7441.184571	14.616141	-0.059808	4.649286
295.459302	7433.253925	14.621146	-0.059826	4.646886
295.209997	7425.186165	14.626151	-0.059774	4.644443
295.359919	7417.248399	14.631155	-0.059797	4.642038
295.130013	7409.176881	14.636160	-0.059749	4.639592
295.315879	7401.246433	14.641165	-0.059778	4.637187
295.344059	7393.233333	14.646170	-0.059778	4.634755
295.118711	7385.169518	14.651175	-0.059731	4.632307
295.104942	7377.173059	14.656179	-0.059723	4.629878
295.219682	7369.129627	14.661184	-0.059740	4.627434
295.340451	7361.167401	14.666189	-0.059757	4.625013
294.913006	7353.217011	14.671194	-0.059672	4.622594
295.124342	7345.150421	14.676199	-0.059706	4.620139
295.257794	7337.232509	14.681203	-0.059726	4.617727
295.057285	7329.197708	14.686208	-0.059683	4.615279
294.781242	7321.157010	14.691213	-0.059627	4.612827
294.913493	7313.155468	14.696218	-0.059646	4.610387
294.905862	7305.126453	14.701223	-0.059640	4.607936
294.808317	7297.135491	14.706227	-0.059616	4.605496
294.833113	7289.183465	14.711232	-0.059616	4.603066
294.819549	7281.135607	14.716237	-0.059608	4.600606
294.749894	7273.222747	14.721242	-0.059590	4.598186
294.662544	7265.163158	14.726247	-0.059568	4.595720
294.649339	7257.170016	14.731251	-0.059561	4.593272
294.418356	7249.062293	14.736256	-0.059512	4.590789
294.391335	7241.094122	14.741261	-0.059502	4.588346
294.485424	7233.075012	14.746266	-0.059514	4.585887
294.476443	7225.132623	14.751271	-0.059508	4.583450
294.570488	7217.126108	14.756275	-0.059520	4.580992
294.649370	7209.133047	14.761280	-0.059529	4.578537
294.619198	7201.122210	14.766285	-0.059519	4.576075
294.466718	7193.107945	14.771290	-0.059485	4.573610
294.300179	7185.053477	14.776295	-0.059449	4.571132
294.406570	7177.104941	14.781299	-0.059463	4.568685
294.287829	7169.084412	14.786304	-0.059436	4.566215
294.223891	7161.102508	14.791309	-0.059419	4.563755
294.361587	7153.169702	14.796314	-0.059440	4.561309
294.266245	7145.125717	14.801319	-0.059417	4.558828
294.437885	7137.172978	14.806323	-0.059443	4.556373
294.187650	7129.078816	14.811328	-0.059392	4.553873
294.226456	7121.053500	14.816333	-0.059394	4.551393
294.203598	7113.086358	14.821338	-0.059384	4.548930
294.054538	7105.097958	14.826343	-0.059351	4.546459
294.345733	7097.089457	14.831347	-0.059400	4.543980
294.063212	7089.147825	14.836352	-0.059342	4.541521
293.973948	7081.103751	14.841357	-0.059321	4.539028
294.186569	7073.133848	14.846362	-0.059355	4.536557
294.212461	7065.085828	14.851367	-0.059355	4.534061
293.901148	7057.121781	14.856371	-0.059291	4.531589
293.761003	7049.093766	14.861376	-0.059260	4.529096
293.954890	7041.117239	14.866381	-0.059291	4.526618
293.941524	7033.095226	14.871386	-0.059283	4.524124
293.828619	7025.121496	14.876391	-0.059257	4.521643
293.932769	7017.139595	14.881395	-0.059271	4.519160
293.817643	7009.126589	14.886400	-0.059245	4.516664
293.726602	7001.088831	14.891405	-0.059223	4.514160
293.765265	6993.029535	14.896410	-0.059225	4.511647
293.537535	6985.002869	14.901415	-0.059177	4.509143
293.537264	6977.056903	14.906419	-0.059172	4.506663
293.410698	6969.056406	14.911424	-0.059143	4.504165
293.497786	6961.061570	14.916429	-0.059154	4.501667
293.374151	6953.091963	14.921434	-0.059126	4.499176
293.318222	6945.067347	14.926439	-0.059110	4.496665
293.451981	6937.046502	14.931443	-0.059130	4.494156
293.317867	6929.024624	14.936448	-0.059100	4.491643
293.288764	6920.985373	14.941453	-0.059089	4.489125
293.270443	6913.054094	14.946458	-0.059080	4.486638
293.343534	6905.053679	14.951463	-0.059089	4.484129
293.204318	6897.059871	14.956467	-0.059058	4.481620
293.247168	6889.061766	14.961472	-0.059061	4.479109
293.248255	6881.049703	14.966477	-0.059056	4.476591
293.098625	6873.074545	14.971482	-0.059023	4.474084
292.914195	6864.989202	14.976487	-0.058983	4.471540
293.044297	6857.018105	14.981491	-0.059002	4.469032
292.945655	6848.988607	14.986496	-0.058978	4.466503
292.918624	6841.008447	14.991501	-0.058968	4.463988
292.967364	6833.026969	14.996506	-0.058972	4.461472
293.012260	6825.028258	15.001511	-0.058975	4.458950
293.167185	6817.045594	15.006515	-0.058999	4.456431
293.010156	6809.005983	15.011520	-0.058964	4.453891
293.104813	6800.966905	15.016525	-0.058977	4.451351
292.920280	6792.986265	15.021530	-0.058937	4.448828
292.843999	6785.012792	15.026535	-0.058918	4.446305
292.848393	6777.006345	15.031539	-0.058914	4.443771
292.833726	6769.034289	15.036544	-0.058906	4.441246
292.563425	6761.007173	15.041549	-0.058850	4.438701
292.718944	6753.041980	15.046554	-0.058874	4.436177
292.594514	6744.955268	15.051559	-0.058845	4.433611
292.602784	6736.949115	15.056563	-0.058842	4.431069
292.410234	6728.938618	15.061568	-0.058801	4.428524
292.519236	6720.940256	15.066573	-0.058816	4.425983
292.619212	6712.968179	15.071578	-0.058829	4.423449
292.576003	6704.954687	15.076583	-0.058816	4.420899
292.384798	6696.986295	15.081587	-0.058775	4.418361
292.387675	6688.979447	15.086592	-0.058771	4.415811
292.249998	6680.942178	15.091597	-0.058740	4.413249
292.280109	6672.968689	15.096602	-0.058740	4.410706
292.331796	6664.930983	15.101607	-0.058745	4.408142
292.424674	6656.928568	15.106611	-0.058757	4.405587
292.121797	6648.986978	15.111616	-0.058695	4.403049
292.288616	6640.959429	15.116621	-0.058721	4.400484
292.195949	6633.012029	15.121626	-0.058699	4.397942
292.076387	6624.979014	15.126631	-0.058671	4.395370
291.954775	6616.947866	15.131635	-0.058643	4.392798
291.975796	6608.891763	15.136640	-0.058642	4.390217
291.969451	6600.937256	15.141645	-0.058636	4.387667
292.001134	6592.963366	15.146650	-0.058636	4.385109
291.859310	6584.988439	15.151655	-0.058605	4.382549
291.931626	6576.985253	15.156659	-0.058613	4.379979
291.811528	6569.015473	15.161664	-0.058585	4.377418
291.769026	6560.964544	15.166669	-0.058572	4.374829
291.870293	6552.990453	15.171674	-0.058586	4.372264
291.759488	6544.918310	15.176679	-0.058560	4.369665
291.962782	6536.971074	15.181683	-0.058593	4.367107
291.763137	6528.944091	15.186688	-0.058550	4.364519
291.755689	6520.975365	15.191693	-0.058544	4.361949
291.710098	6512.998545	15.196698	-0.058530	4.359375
291.659042	6505.011102	15.201703	-0.058515	4.356796
291.638058	6496.965022	15.206707	-0.058506	4.354196
291.454008	6488.861368	15.211712	-0.058467	4.351576
291.397709	6480.845014	15.216717	-0.058451	4.348983
291.486755	6472.926948	15.221722	-0.058463	4.346421
291.239500	6464.909606	15.226727	-0.058411	4.343823
291.309553	6456.946441	15.231731	-0.058419	4.341243
291.432654	6448.969549	15.236736	-0.058437	4.338658
291.298713	6440.965289	15.241741	-0.058407	4.336060
291.367520	6432.953864	15.246746	-0.058414	4.333460
291.391357	6424.916485	15.251751	-0.058414	4.330850
291.461592	6416.946326	15.256755	-0.058422	4.328260
291.172297	6408.904344	15.261760	-0.058362	4.325643
291.155881	6400.960111	15.266765	-0.058354	4.323058
291.149776	6392.982069	15.271770	-0.058348	4.320461
290.965122	6384.945793	15.276775	-0.058308	4.317841
291.013232	6376.919719	15.281779	-0.058312	4.315225
290.936437	6368.935811	15.286784	-0.058293	4.312621
290.961366	6360.863567	15.291789	-0.058292	4.309986
291.056348	6352.948493	15.296794	-0.058305	4.307402
290.926060	6344.888698	15.301799	-0.058275	4.304768
291.052283	6336.932823	15.306803	-0.058293	4.302167
291.047346	6328.942873	15.311808	-0.058287	4.299553
291.125876	6320.952922	15.316813	-0.058297	4.296938
291.139372	6312.928418	15.321818	-0.058294	4.294310
290.956782	6304.856493	15.326823	-0.058255	4.291663
290.909698	6296.879549	15.331827	-0.058241	4.289046
290.750507	6288.934061	15.336832	-0.058206	4.286437
290.878256	6280.871290	15.341837	-0.058225	4.283791
290.814113	6272.925637	15.346842	-0.058207	4.281180
290.770029	6264.899868	15.351847	-0.058194	4.278541
290.895412	6256.906990	15.356851	-0.058212	4.275912
290.603808	6248.918371	15.361856	-0.058153	4.273280
290.414831	6240.852538	15.366861	-0.058112	4.270622
290.689707	6232.925486	15.371866	-0.058158	4.268011
290.667406	6224.806611	15.376871	-0.058149	4.265333
290.728007	6216.909119	15.381875	-0.058155	4.262728
290.675508	6208.862567	15.386880	-0.058140	4.260070
290.637736	6200.904736	15.391885	-0.058128	4.257441
290.544950	6192.908972	15.396890	-0.058105	4.254796
290.482848	6184.858892	15.401895	-0.058089	4.252133
290.504171	6176.858731	15.406899	-0.058087	4.249485
290.577579	6168.917703	15.411904	-0.058096	4.246855
290.353589	6160.855226	15.416909	-0.058049	4.244181
290.265753	6152.956901	15.421914	-0.058027	4.241560
290.274607	6144.933797	15.426919	-0.058024	4.238898
290.255896	6136.934381	15.431923	-0.058015	4.236241
290.218847	6128.882289	15.436928	-0.058003	4.233566
290.085217	6120.849368	15.441933	-0.057973	4.230893
290.178579	6112.910663	15.446938	-0.057985	4.228253
289.917871	6104.859760	15.451943	-0.057931	4.225570
290.164485	6096.908738	15.456947	-0.057972	4.222924
289.893679	6088.913362	15.461952	-0.057917	4.220256
289.781791	6080.933383	15.466957	-0.057891	4.217594
289.925929	6072.919001	15.471962	-0.057912	4.214920
289.782214	6064.878182	15.476967	-0.057880	4.212234
289.550507	6056.894739	15.481971	-0.057832	4.209563
289.676778	6048.932555	15.486976	-0.057850	4.206902
289.882804	6040.908546	15.491981	-0.057883	4.204219
289.925245	6032.952454	15.496986	-0.057886	4.201556
289.571633	6024.917817	15.501991	-0.057815	4.198860
289.562602	6016.944691	15.506995	-0.057808	4.196187
289.642930	6008.837998	15.512000	-0.057818	4.193469
289.548737	6000.832277	15.517005	-0.057795	4.190780
289.410878	5992.832208	15.522010	-0.057764	4.188092
289.270011	5984.838365	15.527015	-0.057733	4.185403
289.565529	5976.874558	15.532019	-0.057783	4.182728
289.371149	5968.892752	15.537024	-0.057741	4.180040
289.416848	5960.934246	15.542029	-0.057745	4.177360
289.338527	5952.892308	15.547034	-0.057725	4.174649
289.014013	5944.860100	15.552039	-0.057659	4.171937
289.271884	5936.866543	15.557043	-0.057702	4.169243
289.053450	5928.878328	15.562048	-0.057656	4.166543
288.956156	5920.882984	15.567053	-0.057633	4.163841
288.934912	5912.933684	15.572058	-0.057624	4.161153
288.912833	5904.915761	15.577063	-0.057614	4.158440
288.898231	5896.917581	15.582067	-0.057607	4.155733
289.001028	5888.895697	15.587072	-0.057620	4.153017
289.027809	5880.818134	15.592077	-0.057620	4.150279
289.103105	5872.891426	15.597082	-0.057629	4.147591
288.998737	5864.836371	15.602087	-0.057604	4.144856
288.850279	5856.900350	15.607091	-0.057572	4.142159
288.922563	5848.876325	15.612096	-0.057580	4.139433
288.835453	5840.905468	15.617101	-0.057558	4.136721
288.894663	5832.881437	15.622106	-0.057564	4.133991
289.027771	5824.822447	15.627111	-0.057584	4.131248
288.830909	5816.875984	15.632115	-0.057542	4.128538
288.676130	5808.867391	15.637120	-0.057508	4.125806
288.817685	5800.879838	15.642125	-0.057529	4.123082
288.742098	5792.902772	15.647130	-0.057510	4.120357
288.756929	5784.878344	15.652135	-0.057507	4.117616
288.710689	5776.892573	15.657139	-0.057494	4.114885
288.620237	5768.843541	15.662144	-0.057472	4.112130
288.349385	5760.824057	15.667149	-0.057416	4.109381
288.425927	5752.833361	15.672154	-0.057425	4.106645
288.634898	5744.821082	15.677159	-0.057459	4.103901
288.327223	5736.902968	15.682163	-0.057396	4.101181
288.430311	5728.865364	15.687168	-0.057410	4.098423
288.350433	5720.886534	15.692173	-0.057390	4.095681
288.213216	5712.905324	15.697178	-0.057360	4.092936
288.016442	5704.866524	15.702183	-0.057318	4.090169
288.145367	5696.902101	15.707187	-0.057336	4.087429
288.089815	5688.866871	15.712192	-0.057321	4.084661
287.982835	5680.914311	15.717197	-0.057296	4.081918
288.015174	5672.925411	15.722202	-0.057297	4.079163
288.022947	5664.919372	15.727207	-0.057293	4.076401
288.140030	5656.902629	15.732211	-0.057310	4.073633
287.969733	5648.873986	15.737216	-0.057273	4.070856
287.902379	5640.887338	15.742221	-0.057255	4.068093
287.935222	5632.896659	15.747226	-0.057256	4.065329
287.637328	5624.931252	15.752231	-0.057195	4.062566
287.889560	5616.931665	15.757235	-0.057237	4.059797
287.884625	5608.933661	15.762240	-0.057231	4.057024
287.856971	5600.907003	15.767245	-0.057220	4.054238
287.759263	5592.917561	15.772250	-0.057197	4.051462
287.761980	5584.896206	15.777255	-0.057192	4.048675
287.779538	5576.901296	15.782259	-0.057190	4.045895
287.649483	5568.939647	15.787264	-0.057161	4.043123
287.808079	5560.911211	15.792269	-0.057185	4.040330
287.651878	5552.957228	15.797274	-0.057151	4.037556
287.482586	5544.910891	15.802279	-0.057114	4.034747
287.499909	5536.796016	15.807283	-0.057112	4.031916
287.483793	5528.841121	15.812288	-0.057104	4.029138
287.569339	5520.852478	15.817293	-0.057115	4.026348
287.526872	5512.911524	15.822298	-0.057102	4.023571
287.438358	5504.892470	15.827303	-0.057080	4.020763
287.397107	5496.910850	15.832307	-0.057067	4.017968
287.308703	5488.912846	15.837312	-0.057046	4.015164
287.178773	5480.870694	15.842317	-0.057016	4.012342
287.262444	5472.878990	15.847322	-0.057027	4.009539
287.170301	5464.886500	15.852327	-0.057004	4.006731
287.235455	5456.893472	15.857331	-0.057011	4.003924
287.420923	5448.912132	15.862336	-0.057041	4.001120
287.124372	5440.884571	15.867341	-0.056980	3.998290
287.058921	5432.923198	15.872346	-0.056963	3.995486
287.230978	5424.866243	15.877351	-0.056990	3.992650
287.185261	5416.865667	15.882355	-0.056976	3.989828
287.100387	5408.907076	15.887360	-0.056955	3.987018
287.154649	5400.882292	15.892365	-0.056960	3.984185
287.258374	5392.924485	15.897370	-0.056974	3.981375
287.122415	5384.890793	15.902375	-0.056943	3.978531
287.142007	5376.920872	15.907379	-0.056942	3.975711
287.135693	5368.919929	15.912384	-0.056936	3.972878
287.058378	5360.875226	15.917389	-0.056916	3.970025
286.761436	5352.944455	15.922394	-0.056855	3.967208
286.905487	5344.887618	15.927399	-0.056877	3.964351
286.962884	5336.939982	15.932403	-0.056883	3.961529
286.850243	5328.980701	15.937408	-0.056856	3.958698
286.765860	5320.979297	15.942413	-0.056836	3.955851
286.836891	5312.961258	15.947418	-0.056844	3.952999
286.573434	5304.902173	15.952423	-0.056789	3.950124
286.631493	5296.922674	15.957427	-0.056795	3.947280
286.614301	5288.915851	15.962432	-0.056786	3.944424
286.468762	5280.939522	15.967437	-0.056754	3.941574
286.457829	5272.948397	15.972442	-0.056747	3.938720
286.405199	5264.961655	15.977447	-0.056732	3.935864
286.371156	5256.978940	15.982451	-0.056720	3.933007
286.273759	5248.960755	15.987456	-0.056697	3.930135
285.976115	5240.975957	15.992461	-0.056637	3.927269
286.230524	5232.930994	15.997466	-0.056679	3.924389
286.297415	5224.965692	16.002471	-0.056686	3.921533
286.001904	5217.000240	16.007475	-0.056626	3.918667
285.998156	5208.999815	16.012480	-0.056620	3.915792
286.134799	5200.926051	16.017485	-0.056640	3.912892
286.433929	5192.918392	16.022490	-0.056691	3.910016
286.188517	5184.958448	16.027495	-0.056640	3.907145
286.032914	5176.975569	16.032499	-0.056606	3.904265
286.030479	5168.974255	16.037504	-0.056600	3.901379
285.871324	5160.995688	16.042509	-0.056565	3.898497
286.131194	5153.007214	16.047514	-0.056608	3.895617
285.962357	5144.958132	16.052519	-0.056572	3.892704
285.784027	5136.926869	16.057523	-0.056533	3.889796
285.677085	5128.985856	16.062528	-0.056508	3.886919
285.681914	5120.944905	16.067533	-0.056504	3.884006
285.629337	5112.995691	16.072538	-0.056489	3.881123
285.600472	5105.008134	16.077543	-0.056478	3.878225
285.804359	5096.981408	16.082547	-0.056511	3.875314
285.676374	5088.780108	16.087552	-0.056482	3.872332
285.389679	5080.758554	16.092557	-0.056423	3.869410
285.412990	5072.871297	16.097562	-0.056423	3.866540
285.431350	5064.901896	16.102567	-0.056421	3.863638
285.460456	5056.923336	16.107571	-0.056421	3.860731
285.302091	5048.966197	16.112576	-0.056386	3.857825
285.356916	5040.937556	16.117581	-0.056391	3.854896
285.475700	5032.973836	16.122586	-0.056408	3.851989
285.327499	5024.942096	16.127591	-0.056375	3.849050
285.197054	5016.979554	16.132595	-0.056346	3.846135
285.291550	5008.979015	16.137600	-0.056358	3.843207
285.374308	5001.001380	16.142605	-0.056369	3.840286
285.426191	4993.064715	16.147610	-0.056373	3.837377
285.255351	4984.989278	16.152615	-0.056336	3.834410
285.083056	4976.992487	16.157619	-0.056299	3.831470
285.109695	4969.015244	16.162624	-0.056299	3.828539
285.243003	4960.981178	16.167629	-0.056318	3.825587
285.097110	4953.038749	16.172634	-0.056286	3.822660
284.934834	4945.016151	16.177639	-0.056250	3.819701
285.055289	4937.076690	16.182643	-0.056268	3.816777
285.002443	4929.046696	16.187648	-0.056253	3.813813
284.897807	4921.023439	16.192653	-0.056228	3.810849
285.068484	4913.046211	16.197658	-0.056255	3.807905
284.961452	4905.026305	16.202663	-0.056229	3.804936
284.833754	4897.094870	16.207667	-0.056201	3.801998
284.711283	4889.106970	16.212672	-0.056173	3.799037
284.816278	4881.093433	16.217677	-0.056187	3.796069
284.623700	4873.060810	16.222682	-0.056146	3.793085
284.670534	4865.039733	16.227687	-0.056149	3.790108
284.617842	4857.040946	16.232691	-0.056134	3.787135
284.700479	4849.045427	16.237696	-0.056145	3.784164
284.644959	4841.053529	16.242701	-0.056129	3.781189
284.686242	4833.099007	16.247706	-0.056132	3.778227
284.504977	4825.052763	16.252711	-0.056093	3.775224
284.379517	4817.058156	16.257715	-0.056064	3.772239
284.384796	4809.061172	16.262720	-0.056060	3.769254
284.328415	4801.038362	16.267725	-0.056044	3.766255
284.364656	4793.072239	16.272730	-0.056046	3.763277
284.386647	4785.068250	16.277735	-0.056045	3.760283
284.298751	4777.104883	16.282739	-0.056023	3.757298
284.476655	4769.076554	16.287744	-0.056051	3.754293
284.343743	4761.070467	16.292749	-0.056021	3.751287
284.416291	4753.098025	16.297754	-0.056029	3.748296
284.260113	4745.047302	16.302759	-0.055995	3.745268
284.454477	4737.084209	16.307763	-0.056026	3.742278
284.294304	4729.104808	16.312768	-0.055991	3.739272
284.178290	4721.105928	16.317773	-0.055964	3.736256
284.326707	4713.126715	16.322778	-0.055987	3.733252
284.180430	4705.076516	16.327783	-0.055954	3.730212
284.078997	4697.103677	16.332787	-0.055930	3.727200
284.044888	4689.147097	16.337792	-0.055919	3.724193
283.774651	4681.169104	16.342797	-0.055863	3.721169
283.996706	4673.183556	16.347802	-0.055899	3.718153
283.846174	4665.151670	16.352807	-0.055866	3.715107
283.915176	4657.054693	16.357811	-0.055874	3.712039
283.817101	4649.087858	16.362816	-0.055850	3.709014
283.670023	4641.094579	16.367821	-0.055818	3.705975
283.607295	4633.133658	16.372826	-0.055801	3.702949
283.558870	4625.128295	16.377831	-0.055787	3.699903
283.449309	4617.164699	16.382835	-0.055761	3.696869
283.606935	4609.181185	16.387840	-0.055785	3.693832
283.490604	4601.153414	16.392845	-0.055758	3.690768
283.416752	4593.181908	16.397850	-0.055739	3.687724
283.416347	4585.177033	16.402855	-0.055734	3.684667
283.536817	4577.225500	16.407859	-0.055751	3.681631
283.524427	4569.224046	16.412864	-0.055744	3.678570
283.469199	4561.201144	16.417869	-0.055728	3.675497
283.570323	4553.193263	16.422874	-0.055742	3.672431
283.438391	4545.184055	16.427879	-0.055712	3.669356
283.221338	4537.197918	16.432883	-0.055667	3.666285
283.444676	4529.197816	16.437888	-0.055703	3.663218
283.401518	4521.206921	16.442893	-0.055690	3.660145
283.249156	4513.248821	16.447898	-0.055656	3.657079
283.120406	4505.221312	16.452903	-0.055627	3.653984
283.137254	4497.204501	16.457907	-0.055625	3.650894
283.171001	4489.217588	16.462912	-0.055626	3.647814
283.092915	4481.190927	16.467917	-0.055606	3.644713
283.017811	4473.262999	16.472922	-0.055587	3.641648
282.938099	4465.251730	16.477927	-0.055567	3.638547
282.737488	4457.283910	16.482931	-0.055525	3.635458
282.884277	4449.223144	16.487936	-0.055547	3.632339
282.921584	4441.199392	16.492941	-0.055548	3.629229
282.782357	4433.231006	16.497946	-0.055517	3.626132
282.705718	4425.240210	16.502951	-0.055498	3.623027
282.806986	4417.235800	16.507955	-0.055512	3.619918
282.867520	4409.282799	16.512960	-0.055518	3.616825
282.512993	4401.262473	16.517965	-0.055446	3.613692
282.811352	4393.243131	16.522970	-0.055497	3.610575
282.527451	4385.299074	16.527975	-0.055439	3.607468
282.482875	4377.286629	16.532979	-0.055425	3.604339
282.542858	4369.348782	16.537984	-0.055431	3.601239
282.501724	4361.318855	16.542989	-0.055418	3.598097
282.360833	4353.354138	16.547994	-0.055387	3.594975
282.548801	4345.309847	16.552999	-0.055417	3.591829
282.509582	4337.286511	16.558003	-0.055404	3.588682
282.397264	4329.347080	16.563008	-0.055378	3.585562
282.106420	4321.365584	16.568013	-0.055319	3.582419
282.398439	4313.338568	16.573018	-0.055368	3.579271
282.459323	4305.382904	16.578023	-0.055374	3.576142
282.275723	4297.360127	16.583027	-0.055335	3.572977
282.235221	4289.366525	16.588032	-0.055322	3.569825
282.086460	4281.382420	16.593037	-0.055289	3.566670
281.982333	4273.385571	16.598042	-0.055265	3.563509
281.879844	4265.422593	16.603047	-0.055240	3.560359
281.881143	4257.402239	16.608051	-0.055235	3.557186
282.105867	4249.380351	16.613056	-0.055272	3.554016
281.818389	4241.313074	16.618061	-0.055213	3.550811
282.036659	4233.346089	16.623066	-0.055249	3.547657
281.925721	4225.334471	16.628071	-0.055223	3.544473
282.033787	4217.378867	16.633075	-0.055238	3.541314
281.910190	4209.383394	16.638080	-0.055210	3.538131
281.940536	4201.372605	16.643085	-0.055210	3.534942
281.878446	4193.416743	16.648090	-0.055193	3.531771
281.702533	4185.428170	16.653095	-0.055155	3.528579
281.691717	4177.396067	16.658099	-0.055148	3.525373
281.570743	4169.467145	16.663104	-0.055120	3.522201
281.550854	4161.467480	16.668109	-0.055112	3.519001
281.615885	4153.479523	16.673114	-0.055119	3.515806
281.643932	4145.459580	16.678119	-0.055119	3.512594
281.448589	4137.438464	16.683123	-0.055077	3.509371
281.264386	4129.460493	16.688128	-0.055037	3.506163
281.626765	4121.443784	16.693133	-0.055100	3.502954
281.653168	4113.466503	16.698138	-0.055099	3.499747
281.330043	4105.531429	16.703143	-0.055034	3.496543
281.503293	4097.493090	16.708147	-0.055061	3.493310
281.494243	4089.510400	16.713152	-0.055054	3.490091
281.488875	4081.486086	16.718157	-0.055048	3.486852
281.402348	4073.558255	16.723162	-0.055027	3.483647
281.365056	4065.568295	16.728167	-0.055015	3.480415
281.301544	4057.569341	16.733171	-0.054998	3.477176
281.294336	4049.584210	16.738176	-0.054991	3.473941
281.209844	4041.524145	16.743181	-0.054970	3.470670
281.235109	4033.542969	16.748186	-0.054970	3.467431
280.992797	4025.572876	16.753191	-0.054919	3.464186
280.956957	4017.564731	16.758195	-0.054908	3.460928
281.035010	4009.606404	16.763200	-0.054917	3.457692
280.779365	4001.575787	16.768205	-0.054864	3.454412
280.911600	3993.571482	16.773210	-0.054884	3.451152
280.784893	3985.603957	16.778215	-0.054855	3.447896
280.629495	3977.607387	16.783219	-0.054821	3.444624
280.741268	3969.655618	16.788224	-0.054836	3.441375
280.856051	3961.615009	16.793229	-0.054852	3.438088
280.659223	3953.651566	16.798234	-0.054811	3.434819
280.476687	3945.631482	16.803239	-0.054771	3.431523
280.471805	3937.610752	16.808243	-0.054765	3.428231
280.552826	3929.620315	16.813248	-0.054775	3.424950
280.569733	3921.646560	16.818253	-0.054773	3.421671
280.488571	3913.660473	16.823258	-0.054753	3.418380
280.674813	3905.660055	16.828263	-0.054782	3.415090
280.573816	3897.644875	16.833267	-0.054758	3.411780
280.500380	3889.682097	16.838272	-0.054740	3.408490
280.377553	3881.691134	16.843277	-0.054711	3.405183
280.497826	3873.751111	16.848282	-0.054729	3.401902
280.471926	3865.754787	16.853287	-0.054719	3.398590
280.354406	3857.744580	16.858291	-0.054692	3.395266
280.633299	3849.672934	16.863296	-0.054738	3.391927
280.241004	3841.687317	16.868301	-0.054660	3.388596
280.081878	3833.715615	16.873306	-0.054625	3.385277
280.107141	3825.757238	16.878311	-0.054625	3.381966
279.943075	3817.759743	16.883315	-0.054589	3.378629
280.137714	3809.785456	16.888320	-0.054620	3.375311
280.140973	3801.743980	16.893325	-0.054616	3.371955
280.170223	3793.777015	16.898330	-0.054616	3.368627
279.890560	3785.804748	16.903335	-0.054559	3.365283
279.871374	3777.821227	16.908339	-0.054550	3.361940
279.954923	3769.842058	16.913344	-0.054560	3.358600
279.723436	3761.840599	16.918349	-0.054512	3.355235
279.588198	3753.840472	16.923354	-0.054481	3.351871
279.758931	3745.824986	16.928359	-0.054508	3.348509
279.862914	3737.793586	16.933363	-0.054522	3.345133
279.691555	3729.866007	16.938368	-0.054485	3.341789
279.494230	3721.872469	16.943373	-0.054443	3.338411
279.549364	3713.897652	16.948378	-0.054448	3.335048
279.497905	3705.883288	16.953383	-0.054434	3.331661
279.293236	3697.891991	16.958387	-0.054390	3.328274
279.468016	3689.888173	16.963392	-0.054418	3.324893
279.449099	3681.917549	16.968397	-0.054409	3.321515
279.482938	3673.941571	16.973402	-0.054410	3.318133
279.328764	3665.969736	16.978407	-0.054376	3.314742
279.237646	3657.938885	16.983411	-0.054354	3.311326
279.254543	3649.945661	16.988416	-0.054352	3.307925
279.291233	3641.911269	16.993421	-0.054354	3.304505
279.138496	3633.992813	16.998426	-0.054320	3.301123
279.171014	3626.005324	17.003431	-0.054321	3.297716
279.131321	3617.990177	17.008435	-0.054308	3.294290
279.098822	3610.000257	17.013440	-0.054297	3.290871
279.082495	3602.008459	17.018445	-0.054289	3.287449
279.120569	3594.042667	17.023450	-0.054291	3.284037
278.985301	3586.065869	17.028455	-0.054260	3.280610
278.966208	3578.078252	17.033459	-0.054252	3.277179
278.909168	3570.086483	17.038464	-0.054236	3.273741
278.867896	3562.050955	17.043469	-0.054223	3.270281
278.911998	3554.054572	17.048474	-0.054226	3.266838
278.820965	3546.081821	17.053479	-0.054204	3.263396
278.779626	3538.087691	17.058483	-0.054191	3.259943
278.727805	3530.154276	17.063488	-0.054176	3.256512
278.636652	3522.110973	17.068493	-0.054154	3.253028
278.602059	3514.120843	17.073498	-0.054142	3.249566
278.670619	3506.142694	17.078503	-0.054150	3.246110
278.658280	3498.141665	17.083507	-0.054142	3.242637
278.664927	3490.172595	17.088512	-0.054138	3.239175
278.560354	3482.198688	17.093517	-0.054114	3.235702
278.599290	3474.136216	17.098522	-0.054116	3.232193
278.619690	3466.145055	17.103527	-0.054114	3.228710
278.398408	3458.162186	17.108531	-0.054068	3.225218
278.389807	3450.216039	17.113536	-0.054061	3.221746
278.290467	3442.206344	17.118541	-0.054037	3.218239
278.315445	3434.217277	17.123546	-0.054037	3.214742
278.214982	3426.236595	17.128551	-0.054013	3.211240
278.243295	3418.245417	17.133555	-0.054013	3.207735
278.305400	3410.262611	17.138560	-0.054020	3.204232
278.223901	3402.282947	17.143565	-0.053999	3.200719
278.201871	3394.318493	17.148570	-0.053990	3.197212
278.006635	3386.326864	17.153575	-0.053948	3.193682
277.891721	3378.298327	17.158579	-0.053922	3.190135
277.901088	3370.330497	17.163584	-0.053918	3.186617
277.811304	3362.352723	17.168589	-0.053896	3.183085
277.985614	3354.355718	17.173594	-0.053924	3.179553
278.013579	3346.381573	17.178599	-0.053924	3.176020
277.912120	3338.371071	17.183603	-0.053900	3.172462
277.990532	3330.377556	17.188608	-0.053909	3.168915
277.724032	3322.386982	17.193613	-0.053854	3.165351
277.957137	3314.418160	17.198618	-0.053892	3.161814
277.891267	3306.449335	17.203623	-0.053875	3.158259
277.570559	3298.467427	17.208627	-0.053810	3.154684
277.526580	3290.456602	17.213632	-0.053797	3.151104
277.413678	3282.429534	17.218637	-0.053770	3.147510
277.255265	3274.471205	17.223642	-0.053736	3.143940
277.091584	3266.505805	17.228647	-0.053700	3.140363
277.288281	3258.489851	17.233651	-0.053732	3.136775
277.534714	3250.485722	17.238656	-0.053772	3.133190
277.336414	3242.493527	17.243661	-0.053730	3.129587
277.397089	3234.530112	17.248666	-0.053736	3.126004
277.240875	3226.572337	17.253671	-0.053702	3.122410
277.257796	3218.587283	17.258675	-0.053700	3.118808
277.155683	3210.636395	17.263680	-0.053676	3.115211
276.972199	3202.610408	17.268685	-0.053636	3.111572
277.154886	3194.600112	17.273690	-0.053665	3.107953
277.140974	3186.599428	17.278695	-0.053657	3.104325
277.233285	3178.639406	17.283699	-0.053669	3.100716
277.089944	3170.678597	17.288704	-0.053638	3.097091
277.055617	3162.664796	17.293709	-0.053626	3.093444
277.159179	3154.648640	17.298714	-0.053640	3.089797
277.044926	3146.700812	17.303719	-0.053614	3.086167
276.727832	3138.726860	17.308723	-0.053549	3.082511
276.663971	3130.767603	17.313728	-0.053532	3.078870
276.661252	3122.772737	17.318733	-0.053527	3.075210
276.578408	3114.698167	17.323738	-0.053506	3.071506
276.452762	3106.711867	17.328743	-0.053477	3.067837
276.471877	3098.713629	17.333747	-0.053476	3.064163
276.614932	3090.746905	17.338752	-0.053497	3.060506
276.648811	3082.759478	17.343757	-0.053498	3.056830
276.516984	3074.810152	17.348762	-0.053469	3.053159
276.562098	3066.809003	17.353767	-0.053472	3.049469
276.443890	3058.838392	17.358771	-0.053445	3.045780
276.356442	3050.881743	17.363776	-0.053423	3.042094
276.315711	3042.886174	17.368781	-0.053411	3.038388
276.444744	3034.898273	17.373786	-0.053429	3.034690
276.362715	3026.920445	17.378791	-0.053409	3.030981
276.299980	3018.931630	17.383795	-0.053392	3.027264
276.504388	3010.935564	17.388800	-0.053425	3.023551
276.221615	3002.953857	17.393805	-0.053367	3.019817
276.300640	2994.987140	17.398810	-0.053377	3.016103
276.219929	2987.006859	17.403815	-0.053356	3.012371
275.944854	2979.018891	17.408819	-0.053300	3.008620
276.113200	2971.019063	17.413824	-0.053326	3.004881
276.084978	2963.049807	17.418829	-0.053316	3.001142
276.156158	2955.056756	17.423834	-0.053324	2.997393
276.018176	2947.091797	17.428839	-0.053293	2.993641
275.866208	2939.073426	17.433843	-0.053259	2.989859
275.996732	2931.086285	17.438848	-0.053279	2.986100
275.947769	2923.092507	17.443853	-0.053264	2.982325
275.885823	2915.132709	17.448858	-0.053248	2.978561
276.010975	2907.161074	17.453863	-0.053266	2.974795
275.851010	2899.159465	17.458867	-0.053231	2.970996
275.703730	2891.208913	17.463872	-0.053198	2.967218
275.799502	2883.203089	17.468877	-0.053211	2.963420
275.669202	2875.236358	17.473882	-0.053181	2.959624
275.507316	2867.312143	17.478887	-0.053146	2.955843
275.442283	2859.261423	17.483891	-0.053129	2.952001
275.705060	2851.258351	17.488896	-0.053172	2.948194
275.491836	2843.263466	17.493901	-0.053127	2.944361
275.215978	2835.356941	17.498906	-0.053071	2.940562
275.425462	2827.370322	17.503911	-0.053105	2.936745
275.307795	2819.327496	17.508915	-0.053078	2.932879
275.405172	2811.356956	17.513920	-0.053091	2.929054
275.384142	2803.368854	17.518925	-0.053082	2.925209
275.337927	2795.428340	17.523930	-0.053068	2.921381
275.288423	2787.453998	17.528935	-0.053053	2.917531
275.047404	2779.444058	17.533939	-0.053003	2.913649
275.266438	2771.371126	17.538944	-0.053039	2.909755
275.009932	2763.414717	17.543949	-0.052986	2.905888
274.908890	2755.502060	17.548954	-0.052962	2.902045
275.111765	2747.495044	17.553959	-0.052995	2.898167
275.092427	2739.517465	17.558963	-0.052986	2.894286
275.041830	2731.541248	17.563968	-0.052971	2.890399
274.797830	2723.567203	17.568973	-0.052921	2.886498
274.926326	2715.583063	17.573978	-0.052939	2.882606
274.823884	2707.629000	17.578983	-0.052915	2.878712
274.662706	2699.652171	17.583987	-0.052880	2.874797
274.818853	2691.634888	17.588992	-0.052904	2.870875
274.672509	2683.663644	17.593997	-0.052871	2.866953
274.742493	2675.690526	17.599002	-0.052879	2.863038
274.528362	2667.730440	17.604007	-0.052834	2.859107
274.597660	2659.721013	17.609011	-0.052842	2.855162
274.583605	2651.745926	17.614016	-0.052834	2.851224
274.466752	2643.747412	17.619021	-0.052807	2.847264
274.558916	2635.799448	17.624026	-0.052819	2.843335
274.367595	2627.849258	17.629031	-0.052778	2.839383
274.329976	2619.877695	17.634035	-0.052766	2.835423
274.401693	2611.865935	17.639040	-0.052774	2.831445
274.361778	2603.854306	17.644045	-0.052762	2.827454
274.202245	2595.893951	17.649050	-0.052727	2.823477
274.236699	2587.929588	17.654055	-0.052728	2.819503
274.082316	2579.972482	17.659059	-0.052694	2.815516
274.022747	2571.977214	17.664064	-0.052678	2.811510
273.939681	2563.981140	17.669069	-0.052657	2.807496
273.814499	2556.019416	17.674074	-0.052629	2.803492
273.795985	2548.053730	17.679079	-0.052620	2.799485
273.642630	2540.094588	17.684083	-0.052586	2.795469
273.904243	2532.064917	17.689088	-0.052630	2.791435
274.050493	2524.053284	17.694093	-0.052652	2.787398
273.756718	2516.115989	17.699098	-0.052592	2.783367
273.714845	2508.169681	17.704103	-0.052579	2.779340
273.782287	2500.181579	17.709107	-0.052586	2.775293
273.813862	2492.193920	17.714112	-0.052587	2.771238
273.625784	2484.215395	17.719117	-0.052547	2.767168
273.571112	2476.250853	17.724122	-0.052532	2.763108
273.496110	2468.301042	17.729127	-0.052512	2.759048
273.263286	2460.337548	17.734131	-0.052464	2.754965
273.424975	2452.248727	17.739136	-0.052489	2.750836
273.387508	2444.286138	17.744141	-0.052477	2.746753
273.132798	2436.340381	17.749146	-0.052424	2.742660
273.167878	2428.369331	17.754151	-0.052425	2.738565
273.409542	2420.365110	17.759155	-0.052465	2.734460
273.559011	2412.377052	17.764160	-0.052488	2.730351
273.241806	2404.449732	17.769165	-0.052424	2.726239
273.095874	2396.488225	17.774170	-0.052391	2.722113
273.121042	2388.534739	17.779175	-0.052391	2.717996
273.317473	2380.519912	17.784179	-0.052422	2.713851
273.106499	2372.548516	17.789184	-0.052378	2.709697
273.063864	2364.565701	17.794189	-0.052365	2.705541
273.008732	2356.605055	17.799194	-0.052349	2.701390
272.960433	2348.653462	17.804199	-0.052335	2.697237
272.933029	2340.660295	17.809203	-0.052325	2.693058
272.806161	2332.701074	17.814208	-0.052296	2.688883
272.703093	2324.716305	17.819213	-0.052272	2.684691
272.715991	2316.772815	17.824218	-0.052269	2.680520
272.942416	2308.781412	17.829223	-0.052306	2.676332
272.592086	2300.811949	17.834227	-0.052235	2.672111
272.690377	2292.812590	17.839232	-0.052248	2.667897
272.632704	2284.837117	17.844237	-0.052233	2.663679
272.578153	2276.860371	17.849242	-0.052217	2.659454
272.395050	2268.934975	17.854247	-0.052178	2.655241
272.523696	2260.900712	17.859251	-0.052197	2.650983
272.624811	2252.947467	17.864256	-0.052210	2.646760
272.276886	2245.002198	17.869261	-0.052140	2.642505
272.224504	2237.042093	17.874266	-0.052125	2.638255
272.259073	2229.074513	17.879271	-0.052127	2.634000
272.223753	2221.037480	17.884275	-0.052115	2.629696
272.393117	2213.076507	17.889280	-0.052141	2.625439
272.390619	2205.115608	17.894285	-0.052136	2.621164
272.223206	2197.175934	17.899290	-0.052099	2.616882
272.107254	2189.211991	17.904295	-0.052073	2.612584
271.945391	2181.228770	17.909299	-0.052037	2.608265
272.210450	2173.247306	17.914304	-0.052081	2.603968
272.137453	2165.286117	17.919309	-0.052063	2.599653
272.084049	2157.340918	17.924314	-0.052048	2.595340
272.114390	2149.189474	17.929319	-0.052048	2.590914
271.947637	2141.218480	17.934323	-0.052012	2.586565
271.843421	2133.314666	17.939328	-0.051987	2.582250
271.830680	2125.360933	17.944333	-0.051980	2.577906
271.793173	2117.402335	17.949338	-0.051967	2.573551
271.781895	2109.449938	17.954343	-0.051960	2.569193
271.605869	2101.493732	17.959347	-0.051922	2.564815
271.608900	2093.562640	17.964352	-0.051918	2.560455
271.567330	2085.597161	17.969357	-0.051905	2.556066
271.587890	2077.597644	17.974362	-0.051903	2.551654
271.556464	2069.630678	17.979367	-0.051892	2.547250
271.392211	2061.679172	17.984371	-0.051857	2.542837
271.555231	2053.711718	17.989376	-0.051882	2.538431
271.354258	2045.757226	17.994381	-0.051839	2.533998
271.141809	2037.788243	17.999386	-0.051794	2.529549
271.086331	2029.836836	18.004391	-0.051779	2.525112
271.301157	2021.843309	18.009395	-0.051814	2.520664
271.379585	2013.890171	18.014400	-0.051823	2.516221
271.018412	2005.934851	18.019405	-0.051751	2.511737
271.041949	1997.923351	18.024410	-0.051750	2.507241
271.161580	1989.957082	18.029415	-0.051767	2.502770
270.954987	1982.029067	18.034419	-0.051724	2.498288
271.216981	1974.032468	18.039424	-0.051767	2.493794
271.076751	1966.066035	18.044429	-0.051736	2.489279
271.014346	1958.110380	18.049434	-0.051719	2.484768
270.935857	1950.183935	18.054439	-0.051699	2.480264
270.864363	1942.234810	18.059443	-0.051681	2.475739
270.814563	1934.255537	18.064448	-0.051666	2.471191
270.739409	1926.274605	18.069453	-0.051647	2.466631
270.605120	1918.324922	18.074458	-0.051617	2.462077
270.678967	1910.370707	18.079463	-0.051626	2.457526
270.553572	1902.402359	18.084467	-0.051597	2.452945
270.469911	1894.434003	18.089472	-0.051576	2.448357
270.421976	1886.475933	18.094477	-0.051562	2.443770
270.536152	1878.511237	18.099482	-0.051578	2.439183
270.369422	1870.578751	18.104487	-0.051542	2.434584
270.268941	1862.520956	18.109491	-0.051518	2.429909
270.470012	1854.550137	18.114496	-0.051550	2.425299
270.335899	1846.625272	18.119501	-0.051520	2.420681
270.376305	1838.674282	18.124506	-0.051523	2.416052
270.378277	1830.716343	18.129511	-0.051518	2.411407
270.132714	1822.761816	18.134515	-0.051467	2.406736
270.052448	1814.826703	18.139520	-0.051447	2.402080
270.032753	1806.868929	18.144525	-0.051438	2.397407
270.039186	1798.901186	18.149530	-0.051434	2.392720
269.980518	1790.940541	18.154535	-0.051418	2.388024
269.849858	1782.979607	18.159539	-0.051388	2.383312
269.867885	1775.037755	18.164544	-0.051387	2.378614
269.814525	1767.080123	18.169549	-0.051372	2.373892
269.703685	1759.107489	18.174554	-0.051346	2.369146
269.751633	1751.149952	18.179559	-0.051350	2.364413
269.788930	1743.196671	18.184563	-0.051351	2.359672
269.815738	1735.268583	18.189568	-0.051351	2.354936
269.720997	1727.269994	18.194573	-0.051328	2.350138
269.547698	1719.312977	18.199578	-0.051291	2.345349
269.515901	1711.384772	18.204583	-0.051280	2.340579
269.658045	1703.400991	18.209587	-0.051301	2.335780
269.746026	1695.427963	18.214592	-0.051312	2.330973
269.663131	1687.495348	18.219597	-0.051292	2.326166
269.338212	1679.578734	18.224602	-0.051226	2.321340
269.443912	1671.640791	18.229607	-0.051241	2.316525
269.415798	1663.640748	18.234611	-0.051230	2.311652
269.315607	1655.702208	18.239616	-0.051206	2.306800
269.210662	1647.744352	18.244621	-0.051182	2.301926
269.218066	1639.798674	18.249626	-0.051178	2.297058
269.216449	1631.848207	18.254631	-0.051172	2.292176
269.094912	1623.870357	18.259635	-0.051145	2.287257
269.296044	1615.927207	18.264640	-0.051177	2.282376
269.096377	1608.018891	18.269645	-0.051135	2.277472
269.036376	1600.027350	18.274650	-0.051118	2.272517
269.041395	1592.029441	18.279655	-0.051114	2.267554
268.943217	1584.084642	18.284659	-0.051091	2.262603
268.722852	1576.176749	18.289664	-0.051044	2.257654
268.627679	1568.233989	18.294669	-0.051021	2.252684
268.799388	1560.239035	18.299674	-0.051048	2.247692
268.677819	1552.322967	18.304679	-0.051020	2.242714
268.564765	1544.384186	18.309683	-0.050994	2.237711
268.651018	1536.433384	18.314688	-0.051005	2.232707
268.774890	1528.438055	18.319693	-0.051023	2.227667
268.606854	1520.519368	18.324698	-0.050987	2.222637
268.722562	1512.588705	18.329703	-0.051003	2.217615
268.695862	1504.626315	18.334707	-0.050993	2.212547
268.708269	1496.680821	18.339712	-0.050990	2.207483
268.494069	1488.755464	18.344717	-0.050945	2.202399
268.442747	1480.836753	18.349722	-0.050930	2.197323
268.378557	1472.896892	18.354727	-0.050913	2.192220
268.077636	1464.942903	18.359731	-0.050852	2.187074
268.117881	1456.993084	18.364736	-0.050854	2.181950
268.230053	1449.039630	18.369741	-0.050870	2.176818
268.062801	1441.091609	18.374746	-0.050834	2.171652
267.880946	1433.169003	18.379751	-0.050795	2.166489
267.801226	1425.227380	18.384755	-0.050775	2.161310
267.965017	1417.286810	18.389760	-0.050800	2.156142
267.796615	1409.352787	18.394765	-0.050764	2.150936
267.755947	1401.391757	18.399770	-0.050751	2.145710
267.747274	1393.458590	18.404775	-0.050744	2.140494
267.713370	1385.525897	18.409779	-0.050733	2.135262
267.936086	1377.546061	18.414784	-0.050769	2.130011
267.736803	1369.632760	18.419789	-0.050727	2.124750
267.865200	1361.691994	18.424794	-0.050745	2.119490
267.697468	1353.791513	18.429799	-0.050709	2.114215
267.712545	1345.764137	18.434803	-0.050707	2.108860
267.563821	1337.851879	18.439808	-0.050674	2.103552
267.377258	1329.957258	18.444813	-0.050634	2.098239
267.261083	1322.026871	18.449818	-0.050607	2.092895
267.408451	1314.070223	18.454823	-0.050629	2.087546
267.260705	1306.147900	18.459827	-0.050597	2.082177
267.291298	1298.238781	18.464832	-0.050597	2.076821
267.154760	1290.295438	18.469837	-0.050567	2.071411
267.324434	1282.320690	18.474842	-0.050593	2.065996
267.274912	1274.419044	18.479847	-0.050579	2.060595
266.886252	1266.532655	18.484851	-0.050501	2.055156
266.876466	1258.587843	18.489856	-0.050494	2.049700
266.733169	1250.667222	18.494861	-0.050463	2.044233
266.627640	1242.756682	18.499866	-0.050438	2.038762
267.049868	1234.766159	18.504871	-0.050511	2.033275
266.887642	1226.819357	18.509875	-0.050476	2.027744
266.877941	1218.910379	18.514880	-0.050469	2.022239
266.638424	1211.017533	18.519885	-0.050419	2.016707
266.751302	1203.056977	18.524890	-0.050435	2.011149
266.577535	1195.158970	18.529895	-0.050397	2.005589
266.418344	1187.250682	18.534899	-0.050363	2.000009
266.484951	1179.329065	18.539904	-0.050370	1.994426
266.376148	1171.388419	18.544909	-0.050345	1.988797
266.167082	1163.485676	18.549914	-0.050301	1.983167
266.515135	1155.527322	18.554919	-0.050360	1.977541
266.416644	1147.604410	18.559923	-0.050337	1.971877
266.196809	1139.716995	18.564928	-0.050291	1.966209
266.120800	1131.800774	18.569933	-0.050271	1.960519
266.048621	1123.897682	18.574938	-0.050253	1.954822
266.083732	1115.925136	18.579943	-0.050254	1.949071
266.142952	1107.980839	18.584947	-0.050260	1.943325
266.170544	1100.075660	18.589952	-0.050260	1.937587
266.011347	1092.176592	18.594957	-0.050225	1.931816
265.860292	1084.256692	18.599962	-0.050192	1.926014
265.809083	1076.373124	18.604967	-0.050177	1.920231
265.678012	1068.462185	18.609971	-0.050148	1.914402
265.628884	1060.537650	18.614976	-0.050133	1.908555
265.812842	1052.591141	18.619981	-0.050163	1.902699
265.762435	1044.695418	18.624986	-0.050148	1.896836
265.546844	1036.815475	18.629991	-0.050103	1.890949
265.500041	1028.885697	18.634995	-0.050089	1.885025
265.447714	1021.014373	18.640000	-0.050074	1.879125
265.523732	1013.083682	18.645005	-0.050083	1.873177
265.286110	1005.165969	18.650010	-0.050034	1.867183
265.475861	997.248326	18.655015	-0.050064	1.861220
265.156355	989.379526	18.660019	-0.049999	1.855215
265.138931	981.454111	18.665024	-0.049991	1.849183
265.165200	973.552731	18.670029	-0.049991	1.843155
265.151722	965.659840	18.675034	-0.049983	1.837109
264.996646	957.773508	18.680039	-0.049949	1.831031
264.974532	949.855792	18.685043	-0.049940	1.824924
265.063420	941.960339	18.690048	-0.049951	1.818828
265.021481	934.070468	18.695053	-0.049938	1.812699
264.763546	926.192831	18.700058	-0.049885	1.806533
265.011511	918.267190	18.705063	-0.049926	1.800370
264.926768	910.383794	18.710067	-0.049905	1.794178
264.725488	902.456997	18.715072	-0.049863	1.787917
264.711469	894.569088	18.720077	-0.049855	1.781687
264.585706	886.698579	18.725082	-0.049826	1.775435
264.405638	878.826888	18.730087	-0.049788	1.769153
264.333605	870.934802	18.735091	-0.049769	1.762846
264.399040	863.055751	18.740096	-0.049776	1.756544
264.446256	855.135403	18.745101	-0.049780	1.750184
264.223932	847.270660	18.750106	-0.049733	1.743812
264.376295	839.376329	18.755111	-0.049757	1.737439
264.244124	831.495181	18.760115	-0.049727	1.731018
264.179393	823.627605	18.765120	-0.049710	1.724593
264.066559	815.783030	18.770125	-0.049684	1.718156
264.042686	807.873708	18.775130	-0.049674	1.711653
264.172765	799.968830	18.780135	-0.049693	1.705149
263.901475	792.134492	18.785139	-0.049638	1.698626
263.943717	784.257689	18.790144	-0.049640	1.692083
264.047133	776.350983	18.795149	-0.049654	1.685499
263.863160	768.517173	18.800154	-0.049615	1.678911
263.762930	760.672062	18.805159	-0.049591	1.672300
263.548059	752.788582	18.810163	-0.049546	1.665614
263.534533	744.939459	18.815168	-0.049539	1.658957
263.497150	737.072698	18.820173	-0.049526	1.652255
263.467820	729.188066	18.825178	-0.049516	1.645512
263.439839	721.359644	18.830183	-0.049506	1.638790
263.360956	713.470753	18.835187	-0.049486	1.631980
263.355762	705.569180	18.840192	-0.049480	1.625142
263.463743	697.705274	18.845197	-0.049495	1.618322
263.398343	689.856780	18.850202	-0.049477	1.611464
263.412265	682.009778	18.855207	-0.049475	1.604588
263.273503	674.178026	18.860211	-0.049444	1.597675
263.087774	666.351860	18.865216	-0.049404	1.590730
262.905172	658.523009	18.870221	-0.049365	1.583752
262.901295	650.671507	18.875226	-0.049359	1.576749
263.060313	642.799491	18.880231	-0.049384	1.569720
262.778983	634.996595	18.885235	-0.049327	1.562657
262.713440	627.181550	18.890240	-0.049309	1.555583
262.880507	619.285310	18.895245	-0.049335	1.548437
262.684910	611.471424	18.900250	-0.049294	1.541279
262.687688	603.649874	18.905255	-0.049289	1.534110
262.699961	595.795099	18.910259	-0.049286	1.526879
262.593190	587.992428	18.915264	-0.049261	1.519643
262.543737	580.175907	18.920269	-0.049247	1.512369
262.245144	572.372749	18.925274	-0.049186	1.505034
262.265050	564.560031	18.930279	-0.049185	1.497703
262.280265	556.718211	18.935283	-0.049183	1.490307
262.209758	548.921348	18.940288	-0.049165	1.482904
262.259586	541.107901	18.945293	-0.049169	1.475467
261.953924	533.273318	18.950298	-0.049107	1.467916
261.927214	525.470868	18.955303	-0.049097	1.460400
261.983654	517.654611	18.960307	-0.049102	1.452846
262.148030	509.816085	18.965312	-0.049128	1.445248
261.893742	502.086821	18.970317	-0.049075	1.437650
261.671346	494.294858	18.975322	-0.049029	1.429954
261.853703	486.476424	18.980327	-0.049058	1.422256
261.626934	478.721248	18.985331	-0.049011	1.414513
261.708561	470.909516	18.990336	-0.049021	1.406721
261.611816	463.161416	18.995341	-0.048998	1.398920
261.304473	455.410443	19.000346	-0.048935	1.391037
261.248338	447.631933	19.005351	-0.048920	1.383123
261.443316	439.815006	19.010355	-0.048951	1.375167
261.273987	432.063751	19.015360	-0.048915	1.367171
261.218033	424.315712	19.020365	-0.048899	1.359150
261.233834	416.530751	19.025370	-0.048897	1.351055
261.364202	408.760502	19.030375	-0.048916	1.342947
261.130189	401.039104	19.035379	-0.048868	1.334777
261.033144	393.294553	19.040384	-0.048844	1.326556
261.068148	385.562210	19.045389	-0.048846	1.318321
260.727709	377.761081	19.050394	-0.048778	1.309892
260.840511	369.972047	19.055399	-0.048793	1.301504
260.761377	362.259805	19.060403	-0.048774	1.293110
260.659879	354.544728	19.065408	-0.048750	1.284654
260.602124	346.854610	19.070413	-0.048734	1.276178
260.329238	339.161948	19.075418	-0.048678	1.267602
260.615725	331.413079	19.080423	-0.048727	1.259010
260.310797	323.743174	19.085427	-0.048665	1.250335
260.304795	316.042276	19.090432	-0.048659	1.241622
260.375007	308.348064	19.095437	-0.048667	1.232870
260.138951	300.671485	19.100442	-0.048618	1.224016
260.177561	292.986815	19.105447	-0.048620	1.215142
259.959738	285.325604	19.110451	-0.048575	1.206179
259.928112	277.670095	19.115456	-0.048564	1.197192
259.871885	270.000232	19.120461	-0.048548	1.188116
259.737465	262.357395	19.125466	-0.048518	1.178986
259.797599	254.698422	19.130471	-0.048524	1.169806
259.616319	247.075530	19.135475	-0.048486	1.160547
259.402307	239.455777	19.140480	-0.048441	1.151210
259.601287	231.767963	19.145485	-0.048473	1.141800
259.449991	224.163918	19.150490	-0.048440	1.132341
259.329387	216.570951	19.155495	-0.048413	1.122823
259.307972	208.962505	19.160499	-0.048404	1.113225
259.212760	201.367653	19.165504	-0.048381	1.103546
259.105142	193.799602	19.170509	-0.048356	1.093812
259.010179	186.223524	19.175514	-0.048333	1.083983
259.137180	178.644226	19.180519	-0.048352	1.074110
258.785876	171.117871	19.185523	-0.048282	1.064107
258.762423	163.567591	19.190528	-0.048273	1.054052
258.704511	156.034671	19.195533	-0.048257	1.043916
258.701275	148.501717	19.200538	-0.048251	1.033693
258.706803	140.979624	19.205543	-0.048248	1.023385
258.543809	133.499424	19.210547	-0.048212	1.012989
258.543063	126.003459	19.215552	-0.048207	1.002504
258.473433	118.525103	19.220557	-0.048189	0.991915
258.338771	111.048601	19.225562	-0.048160	0.981199
258.153033	103.629328	19.230567	-0.048120	0.970434
258.036295	96.196818	19.235571	-0.048094	0.959546
257.845819	88.798621	19.240576	-0.048053	0.948566
257.722623	81.399671	19.245581	-0.048026	0.937473
257.784944	73.984074	19.250586	-0.048032	0.926272
257.747433	66.625477	19.255591	-0.048021	0.914994
257.573053	59.501242	19.260595	-0.047984	0.903903