Fri Mar 12 12:30:19 2021


Number of Points = 3625

Depth (nm)	Load (N)	Time (s)	Disp. Voltage(V)	Force Voltage(V)
1.193875	0.033564	0.000000	-0.000007	0.721317
1.163120	-0.061188	0.005005	-0.000001	0.721120
1.048144	-0.035186	0.010010	0.000020	0.721131
1.103963	-0.049796	0.015014	0.000010	0.721121
1.181079	-0.061849	0.020019	-0.000004	0.721125
1.273910	-0.077534	0.025024	-0.000022	0.721126
0.933729	-0.020237	0.030029	0.000042	0.721120
0.955702	-0.019495	0.035034	0.000038	0.721129
1.220942	-0.071119	0.040038	-0.000012	0.721121
1.190351	-0.064866	0.045043	-0.000006	0.721122
1.092836	-0.046179	0.050048	0.000012	0.721125
1.001556	-0.033959	0.055053	0.000029	0.721117
1.180246	-0.061124	0.060058	-0.000004	0.721126
1.107253	-0.050812	0.065062	0.000009	0.721121
0.996678	-0.031267	0.070067	0.000030	0.721121
1.119884	-0.051171	0.075072	0.000007	0.721125
0.954659	-0.127860	0.080077	0.000038	0.720916
1.228394	-0.194245	0.085082	-0.000013	0.720882
1.314904	-0.210788	0.090086	-0.000030	0.720879
1.273975	-0.205312	0.095091	-0.000022	0.720876
1.171016	-0.185576	0.100096	-0.000003	0.720879
1.049147	-0.168066	0.105101	0.000020	0.720870
1.159928	-0.263374	0.110106	-0.000001	0.720722
1.001147	-0.329693	0.115110	0.000029	0.720536
1.034741	-0.334989	0.120115	0.000023	0.720537
1.206917	-0.362863	0.125120	-0.000010	0.720543
1.044429	-0.339306	0.130125	0.000021	0.720532
1.018962	-0.397314	0.135130	0.000025	0.720409
1.075332	-0.502738	0.140134	0.000015	0.720221
1.130363	-0.511298	0.145139	0.000005	0.720224
1.113764	-0.507259	0.150144	0.000008	0.720226
1.013635	-0.526982	0.155149	0.000026	0.720152
1.062501	-0.663083	0.160154	0.000017	0.719901
1.073349	-0.668844	0.165158	0.000015	0.719894
1.155802	-0.681575	0.170163	-0.000000	0.719897
1.197632	-0.762760	0.175168	-0.000008	0.719752
1.156459	-0.835721	0.180173	-0.000000	0.719594
1.080866	-0.818999	0.185178	0.000014	0.719600
1.112741	-0.854635	0.190182	0.000008	0.719541
1.167872	-1.004885	0.195187	-0.000002	0.719265
1.015225	-0.974797	0.200192	0.000026	0.719270
0.770686	-0.941483	0.205197	0.000072	0.719250
0.974695	-1.123293	0.210202	0.000034	0.718963
0.844747	-1.103816	0.215206	0.000058	0.718956
0.736123	-1.091459	0.220211	0.000078	0.718942
0.944530	-1.278142	0.225216	0.000039	0.718647
0.928602	-1.281541	0.230221	0.000042	0.718635
1.046976	-1.340055	0.235226	0.000020	0.718561
1.019730	-1.442715	0.240230	0.000025	0.718349
1.012022	-1.442595	0.245235	0.000027	0.718347
1.004717	-1.563118	0.250240	0.000028	0.718106
0.706827	-1.560343	0.255245	0.000084	0.718007
0.962318	-1.640088	0.260250	0.000036	0.717939
0.810951	-1.736146	0.265254	0.000064	0.717696
0.646446	-1.705884	0.270259	0.000095	0.717698
0.651273	-1.838326	0.275264	0.000094	0.717438
0.636474	-1.868678	0.280269	0.000097	0.717373
0.665317	-1.941964	0.285274	0.000091	0.717238
0.540765	-2.000027	0.290278	0.000115	0.717079
0.871358	-2.096816	0.295283	0.000053	0.717005
1.034398	-2.251989	0.300288	0.000023	0.716755
0.777723	-2.232718	0.305293	0.000071	0.716703
0.774128	-2.359811	0.310298	0.000071	0.716450
0.824915	-2.388871	0.315302	0.000062	0.716410
0.518326	-2.476676	0.320307	0.000119	0.716128
0.472107	-2.473868	0.325312	0.000128	0.716118
0.351540	-2.573677	0.330317	0.000150	0.715877
-0.251407	-2.462279	0.335322	0.000262	0.715885
-2.521724	-2.223616	0.340326	0.000685	0.715557
-2.858711	-2.170343	0.345331	0.000747	0.715543
-2.802889	-2.179409	0.350336	0.000737	0.715545
-3.020895	-2.271591	0.355341	0.000778	0.715286
-3.667465	-2.182879	0.360346	0.000898	0.715233
-3.989573	-2.128317	0.365350	0.000958	0.715228
-3.891655	-2.190093	0.370355	0.000940	0.715140
-4.386580	-2.219884	0.375360	0.001032	0.714906
-4.647237	-2.179217	0.380365	0.001080	0.714894
-4.818948	-2.142085	0.385370	0.001112	0.714907
-4.662639	-2.215816	0.390374	0.001083	0.714816
-5.809662	-2.120608	0.395379	0.001297	0.714600
-5.260358	-2.213740	0.400384	0.001194	0.714609
-5.726995	-2.137002	0.405389	0.001281	0.714597
-5.612402	-2.151901	0.410394	0.001260	0.714608
-5.884061	-2.241651	0.415398	0.001310	0.714333
-6.591583	-2.146828	0.420403	0.001442	0.714271
-6.309344	-2.195371	0.425408	0.001390	0.714275
-6.524727	-2.161309	0.430413	0.001430	0.714266
-6.475128	-2.167225	0.435418	0.001420	0.714272
-6.840147	-2.258144	0.440422	0.001488	0.713962
-7.542978	-2.133857	0.445427	0.001619	0.713961
-7.666910	-2.107915	0.450432	0.001642	0.713968
-7.086943	-2.216338	0.455437	0.001534	0.713958
-7.101026	-2.209064	0.460442	0.001537	0.713968
-8.064491	-2.165140	0.465446	0.001716	0.713714
-8.584307	-2.106239	0.470451	0.001813	0.713647
-8.141380	-2.182825	0.475456	0.001730	0.713652
-8.415280	-2.137704	0.480461	0.001781	0.713644
-8.431421	-2.131714	0.485466	0.001784	0.713651
-8.263235	-2.164926	0.490470	0.001753	0.713644
-8.863454	-2.172274	0.495475	0.001865	0.713417
-9.392102	-2.107898	0.500480	0.001963	0.713358
-9.268432	-2.133883	0.505485	0.001940	0.713350
-9.089355	-2.162873	0.510490	0.001907	0.713356
-9.399415	-2.110090	0.515494	0.001964	0.713351
-9.245952	-2.136910	0.520499	0.001936	0.713352
-8.886812	-2.278615	0.525504	0.001869	0.713198
-10.588569	-2.068363	0.530509	0.002186	0.713013
-10.044792	-2.161787	0.535514	0.002084	0.713020
-9.900039	-2.188625	0.540518	0.002057	0.713018
-10.479991	-2.086300	0.545523	0.002165	0.713016
-10.285060	-2.117490	0.550528	0.002129	0.713023
-10.262320	-2.126471	0.555533	0.002125	0.713013
-10.443875	-2.228810	0.560538	0.002159	0.712745
-11.202253	-2.114803	0.565542	0.002300	0.712703
-11.333665	-2.092395	0.570547	0.002324	0.712701
-10.906737	-2.165944	0.575552	0.002245	0.712706
-11.243937	-2.109065	0.580557	0.002307	0.712700
-11.126814	-2.125609	0.585562	0.002286	0.712708
-10.825744	-2.200567	0.590566	0.002230	0.712666
-11.843150	-2.163426	0.595571	0.002419	0.712379
-11.777943	-2.170331	0.600576	0.002407	0.712388
-12.004414	-2.135569	0.605581	0.002449	0.712377
-11.856952	-2.156934	0.610586	0.002421	0.712387
-12.018445	-2.131282	0.615590	0.002451	0.712381
-12.008556	-2.133659	0.620595	0.002450	0.712380
-11.616380	-2.266021	0.625600	0.002377	0.712255
-13.236025	-2.064963	0.630605	0.002678	0.712081
-12.945333	-2.113537	0.635610	0.002624	0.712088
-12.712473	-2.156976	0.640614	0.002581	0.712084
-12.828333	-2.136515	0.645619	0.002602	0.712083
-12.919502	-2.117046	0.650624	0.002619	0.712090
-13.071029	-2.093520	0.655629	0.002647	0.712083
-12.867769	-2.181071	0.660634	0.002609	0.711981
-13.824172	-2.125247	0.665638	0.002787	0.711752
-13.801353	-2.129614	0.670643	0.002783	0.711752
-13.770623	-2.131124	0.675648	0.002777	0.711760
-13.839087	-2.121731	0.680653	0.002790	0.711754
-13.780235	-2.129152	0.685658	0.002779	0.711760
-13.693572	-2.146031	0.690662	0.002763	0.711758
-13.808815	-2.162752	0.695667	0.002784	0.711683
-14.611608	-2.133033	0.700672	0.002934	0.711457
-14.370183	-2.180659	0.705677	0.002889	0.711448
-14.380657	-2.176080	0.710682	0.002891	0.711454
-14.690747	-2.122338	0.715686	0.002948	0.711451
-14.699737	-2.121663	0.720691	0.002950	0.711449
-14.453984	-2.161373	0.725696	0.002904	0.711457
-14.722396	-2.182436	0.730701	0.002954	0.711320
-15.682571	-2.101688	0.735706	0.003133	0.711140
-15.223470	-2.185091	0.740710	0.003048	0.711137
-15.312852	-2.169620	0.745715	0.003064	0.711136
-15.564023	-2.122151	0.750720	0.003111	0.711141
-15.479429	-2.142377	0.755725	0.003095	0.711131
-15.246459	-2.178638	0.760730	0.003052	0.711141
-15.294170	-2.253857	0.765734	0.003061	0.710974
-16.567147	-2.080294	0.770739	0.003297	0.710868
-15.845206	-2.206470	0.775744	0.003163	0.710873
-16.079341	-2.168528	0.780749	0.003207	0.710866
-16.467362	-2.096672	0.785754	0.003279	0.710871
-16.203270	-2.145676	0.790758	0.003230	0.710867
-16.254771	-2.138364	0.795763	0.003239	0.710864
-16.676669	-2.224838	0.800768	0.003318	0.710541
-17.068409	-2.163965	0.805773	0.003391	0.710523
-17.102755	-2.153963	0.810778	0.003397	0.710531
-17.028486	-2.166757	0.815782	0.003383	0.710532
-17.479614	-2.089751	0.820787	0.003467	0.710525
-17.116467	-2.149960	0.825792	0.003399	0.710534
-17.201062	-2.154880	0.830797	0.003415	0.710494
-18.175734	-2.121936	0.835802	0.003597	0.710213
-18.223435	-2.113033	0.840806	0.003606	0.710214
-18.150923	-2.127233	0.845811	0.003592	0.710211
-17.904222	-2.167397	0.850816	0.003546	0.710219
-18.380551	-2.088201	0.855821	0.003635	0.710208
-17.984478	-2.155101	0.860826	0.003561	0.710215
-17.892111	-2.171042	0.865830	0.003544	0.710216
-19.027824	-2.103677	0.870835	0.003755	0.709947
-19.251374	-2.089125	0.875840	0.003797	0.709896
-18.816958	-2.171608	0.880845	0.003716	0.709886
-18.963396	-2.142414	0.885850	0.003743	0.709892
-19.209345	-2.100250	0.890854	0.003789	0.709889
-19.166790	-2.110047	0.895859	0.003781	0.709885
-18.915708	-2.149823	0.900864	0.003734	0.709895
-19.337904	-2.121339	0.905869	0.003813	0.709801
-19.800524	-2.141686	0.910874	0.003899	0.709596
-19.573532	-2.185055	0.915878	0.003857	0.709590
-20.316035	-2.051936	0.920883	0.003995	0.709591
-19.834528	-2.134147	0.925888	0.003905	0.709599
-19.625149	-2.177264	0.930893	0.003866	0.709587
-20.185767	-2.074180	0.935898	0.003970	0.709594
-20.045916	-2.133743	0.940902	0.003944	0.709524
-20.584032	-2.171291	0.945907	0.004044	0.709257
-20.410103	-2.197479	0.950912	0.004012	0.709267
-21.325389	-2.040351	0.955917	0.004182	0.709255
-20.741803	-2.141382	0.960922	0.004074	0.709261
-20.527254	-2.179724	0.965926	0.004034	0.709261
-21.150043	-2.070240	0.970931	0.004150	0.709258
-21.132487	-2.075385	0.975936	0.004146	0.709254
-21.510004	-2.159434	0.980941	0.004217	0.708951
-21.818831	-2.101652	0.985946	0.004274	0.708957
-22.111355	-2.050752	0.990950	0.004329	0.708954
-21.528193	-2.155299	0.995955	0.004220	0.708953
-21.390142	-2.176811	1.000960	0.004194	0.708959
-21.966657	-2.078845	1.005965	0.004302	0.708950
-21.793581	-2.105547	1.010970	0.004269	0.708958
-21.894207	-2.208558	1.015974	0.004288	0.708716
-23.135188	-2.029964	1.020979	0.004519	0.708631
-22.831795	-2.081025	1.025984	0.004463	0.708637
-22.547880	-2.132979	1.030989	0.004410	0.708634
-22.830608	-2.080667	1.035994	0.004462	0.708638
-22.910398	-2.066162	1.040998	0.004477	0.708639
-22.741324	-2.100259	1.046003	0.004446	0.708631
-22.699210	-2.144849	1.051008	0.004438	0.708557
-23.928100	-2.031932	1.056013	0.004666	0.708344
-23.555909	-2.096154	1.061018	0.004597	0.708349
-23.291249	-2.143780	1.066022	0.004548	0.708348
-23.429330	-2.122118	1.071027	0.004574	0.708342
-23.383421	-2.126433	1.076032	0.004565	0.708350
-23.527681	-2.102774	1.081037	0.004592	0.708346
-23.438101	-2.175944	1.086042	0.004575	0.708231
-24.572689	-2.083751	1.091046	0.004786	0.708010
-24.289922	-2.136124	1.096051	0.004734	0.708007
-24.293999	-2.130286	1.101056	0.004734	0.708017
-24.596739	-2.081454	1.106061	0.004791	0.708007
-24.556569	-2.086149	1.111066	0.004783	0.708012
-24.369365	-2.119582	1.116070	0.004748	0.708012
-24.338642	-2.167597	1.121075	0.004743	0.707926
-25.282254	-2.112620	1.126080	0.004918	0.707699
-25.121643	-2.146684	1.131085	0.004888	0.707689
-25.514694	-2.072878	1.136090	0.004961	0.707696
-25.511338	-2.074399	1.141094	0.004961	0.707694
-25.266699	-2.118420	1.146099	0.004915	0.707694
-25.205549	-2.125611	1.151104	0.004904	0.707701
-25.653598	-2.052626	1.156109	0.004987	0.707687
-26.082336	-2.132788	1.161114	0.005067	0.707373
-25.940098	-2.158907	1.166118	0.005041	0.707372
-26.348204	-2.090703	1.171123	0.005116	0.707363
-26.387270	-2.077738	1.176128	0.005124	0.707375
-26.374885	-2.084757	1.181133	0.005121	0.707365
-26.230801	-2.109767	1.186138	0.005095	0.707367
-26.298536	-2.097293	1.191142	0.005107	0.707367
-26.842543	-2.109360	1.196147	0.005208	0.707149
-26.842190	-2.145376	1.201152	0.005208	0.707077
-27.022501	-2.118551	1.206157	0.005242	0.707066
-27.066196	-2.106863	1.211162	0.005250	0.707074
-27.339813	-2.059362	1.216166	0.005301	0.707071
-27.349395	-2.058109	1.221171	0.005303	0.707070
-27.061899	-2.104911	1.226176	0.005249	0.707079
-27.305843	-2.167851	1.231181	0.005294	0.706866
-27.845231	-2.130765	1.236186	0.005395	0.706747
-27.934402	-2.114898	1.241190	0.005411	0.706747
-27.921110	-2.119898	1.246195	0.005409	0.706742
-27.697125	-2.154838	1.251200	0.005367	0.706752
-28.093937	-2.088368	1.256205	0.005441	0.706744
-28.347090	-2.040627	1.261210	0.005488	0.706749
-28.026193	-2.210648	1.266214	0.005428	0.706522
-28.984412	-2.083296	1.271219	0.005607	0.706435
-29.080612	-2.060620	1.276224	0.005625	0.706446
-29.086228	-2.063880	1.281229	0.005626	0.706438
-28.798975	-2.112510	1.286234	0.005572	0.706443
-28.733793	-2.123534	1.291238	0.005560	0.706444
-29.157942	-2.051605	1.296243	0.005639	0.706437
-28.731885	-2.217838	1.301248	0.005560	0.706255
-29.662452	-2.117758	1.306253	0.005733	0.706123
-29.470352	-2.150127	1.311258	0.005697	0.706127
-29.502076	-2.143877	1.316262	0.005703	0.706128
-29.930602	-2.072407	1.321267	0.005783	0.706118
-29.798562	-2.090692	1.326272	0.005758	0.706129
-29.551165	-2.137926	1.331277	0.005712	0.706123
-29.713322	-2.234233	1.336282	0.005742	0.705871
-30.381797	-2.120257	1.341286	0.005867	0.705861
-30.990946	-2.013480	1.346291	0.005980	0.705857
-30.242459	-2.143443	1.351296	0.005841	0.705864
-30.208054	-2.154105	1.356301	0.005834	0.705855
-30.671079	-2.069806	1.361306	0.005920	0.705859
-30.343382	-2.194296	1.366310	0.005859	0.705726
-31.315996	-2.124329	1.371315	0.006040	0.705518
-31.076381	-2.163969	1.376320	0.005996	0.705524
-31.640305	-2.067578	1.381325	0.006101	0.705516
-31.544046	-2.083020	1.386330	0.006083	0.705519
-31.127501	-2.157808	1.391334	0.006005	0.705518
-31.477037	-2.099132	1.396339	0.006070	0.705511
-31.307932	-2.222541	1.401344	0.006039	0.705323
-32.288415	-2.109622	1.406349	0.006221	0.705199
-32.414168	-2.083626	1.411354	0.006245	0.705206
-32.232495	-2.115497	1.416358	0.006211	0.705207
-32.413061	-2.085700	1.421363	0.006244	0.705203
-32.217625	-2.114248	1.426368	0.006208	0.705215
-32.469282	-2.076662	1.431373	0.006255	0.705201
-32.297564	-2.189719	1.436378	0.006223	0.705035
-33.183417	-2.107475	1.441382	0.006388	0.704882
-33.379095	-2.076338	1.446387	0.006424	0.704875
-32.896986	-2.158361	1.451392	0.006334	0.704883
-33.076351	-2.128659	1.456397	0.006368	0.704878
-33.139098	-2.114516	1.461402	0.006379	0.704884
-33.261899	-2.093697	1.466406	0.006402	0.704882
-33.268729	-2.176822	1.471411	0.006403	0.704712
-34.054718	-2.098088	1.476416	0.006550	0.704589
-33.986109	-2.113988	1.481421	0.006537	0.704581
-33.967566	-2.116662	1.486426	0.006533	0.704583
-33.856802	-2.134422	1.491430	0.006513	0.704587
-34.139584	-2.088800	1.496435	0.006565	0.704577
-33.866752	-2.131347	1.501440	0.006515	0.704590
-34.189496	-2.189017	1.506445	0.006575	0.704357
-35.337221	-2.034372	1.511450	0.006788	0.704257
-34.849403	-2.119705	1.516454	0.006697	0.704260
-34.937568	-2.107730	1.521459	0.006714	0.704253
-34.786901	-2.131754	1.526464	0.006686	0.704258
-35.039603	-2.090329	1.531469	0.006733	0.704251
-34.784021	-2.134993	1.536474	0.006685	0.704253
-34.722679	-2.231549	1.541478	0.006674	0.704080
-36.339413	-2.011644	1.546483	0.006975	0.703943
-35.829963	-2.097392	1.551488	0.006880	0.703953
-35.426778	-2.175300	1.556493	0.006805	0.703941
-35.810061	-2.104322	1.561498	0.006876	0.703946
-35.866968	-2.093391	1.566502	0.006887	0.703948
-35.693588	-2.125568	1.571507	0.006854	0.703945
-35.677071	-2.222217	1.576512	0.006851	0.703756
-36.927652	-2.063649	1.581517	0.007084	0.703627
-36.889951	-2.070204	1.586522	0.007077	0.703627
-36.484184	-2.140255	1.591526	0.007001	0.703632
-37.046741	-2.044277	1.596531	0.007106	0.703623
-36.771482	-2.087849	1.601536	0.007055	0.703634
-36.657548	-2.111787	1.606541	0.007034	0.703627
-36.669841	-2.164893	1.611546	0.007036	0.703515
-37.774443	-2.055639	1.616550	0.007241	0.703338
-37.552820	-2.098776	1.621555	0.007200	0.703331
-37.482225	-2.104740	1.626560	0.007187	0.703345
-37.526802	-2.101497	1.631565	0.007195	0.703335
-37.576904	-2.092398	1.636570	0.007205	0.703336
-37.488820	-2.104805	1.641574	0.007188	0.703342
-37.947345	-2.070053	1.646579	0.007273	0.703247
-38.507177	-2.090354	1.651584	0.007378	0.703005
-38.237906	-2.140826	1.656589	0.007328	0.703000
-38.726814	-2.052097	1.661594	0.007419	0.703003
-38.630106	-2.068633	1.666598	0.007401	0.703005
-38.474345	-2.100683	1.671603	0.007372	0.702996
-38.178555	-2.148232	1.676608	0.007316	0.703007
-38.582523	-2.097254	1.681613	0.007392	0.702964
-39.600440	-2.051894	1.686618	0.007581	0.702689
-39.364085	-2.093832	1.691622	0.007537	0.702690
-39.721674	-2.034002	1.696627	0.007604	0.702682
-39.384595	-2.089226	1.701632	0.007541	0.702692
-39.394105	-2.089604	1.706637	0.007543	0.702688
-39.458230	-2.075842	1.711642	0.007554	0.702692
-39.495178	-2.069165	1.716646	0.007561	0.702693
-39.468291	-2.171929	1.721651	0.007556	0.702495
-40.355417	-2.074011	1.726656	0.007721	0.702373
-40.313068	-2.086570	1.731661	0.007714	0.702363
-40.456571	-2.059426	1.736666	0.007740	0.702366
-40.212088	-2.100189	1.741670	0.007695	0.702372
-40.504986	-2.050925	1.746675	0.007749	0.702366
-40.515588	-2.046282	1.751680	0.007751	0.702371
-40.491866	-2.104702	1.756685	0.007747	0.702262
-41.227947	-2.069043	1.761690	0.007884	0.702069
-40.893126	-2.127499	1.766694	0.007821	0.702071
-41.237831	-2.069766	1.771699	0.007885	0.702064
-40.846446	-2.135452	1.776704	0.007813	0.702072
-40.927067	-2.123072	1.781709	0.007828	0.702068
-41.498261	-2.022060	1.786714	0.007934	0.702067
-40.916343	-2.221078	1.791718	0.007826	0.701874
-42.308607	-2.042127	1.796723	0.008085	0.701734
-42.171008	-2.062023	1.801728	0.008059	0.701743
-42.058330	-2.085691	1.806733	0.008038	0.701736
-42.060530	-2.083668	1.811738	0.008038	0.701739
-41.952176	-2.101241	1.816742	0.008018	0.701743
-42.403783	-2.024173	1.821747	0.008102	0.701736
-42.318248	-2.099657	1.826752	0.008086	0.701614
-43.045030	-2.061588	1.831757	0.008222	0.701429
-42.976696	-2.071949	1.836762	0.008209	0.701433
-42.670084	-2.124955	1.841766	0.008152	0.701436
-43.017135	-2.066875	1.846771	0.008216	0.701428
-42.838495	-2.094824	1.851776	0.008183	0.701436
-43.003132	-2.067922	1.856781	0.008214	0.701431
-42.594104	-2.219259	1.861786	0.008138	0.701273
-43.761326	-2.086686	1.866790	0.008355	0.701120
-43.896182	-2.066557	1.871795	0.008380	0.701112
-43.505157	-2.131072	1.876800	0.008307	0.701123
-43.590067	-2.120081	1.881805	0.008323	0.701114
-43.971627	-2.052877	1.886810	0.008394	0.701113
-43.701581	-2.098400	1.891814	0.008344	0.701118
-44.006588	-2.138476	1.896819	0.008400	0.700927
-44.705138	-2.038667	1.901824	0.008530	0.700877
-44.472765	-2.084176	1.906829	0.008487	0.700868
-44.064357	-2.158189	1.911834	0.008411	0.700866
-44.143777	-2.142050	1.916838	0.008426	0.700870
-44.584306	-2.064714	1.921843	0.008508	0.700868
-44.266745	-2.184348	1.926848	0.008449	0.700740
-45.253833	-2.111822	1.931853	0.008632	0.700530
-45.228032	-2.116835	1.936858	0.008628	0.700530
-45.115026	-2.135860	1.941862	0.008606	0.700532
-45.258264	-2.114424	1.946867	0.008633	0.700524
-45.194035	-2.119822	1.951872	0.008621	0.700536
-45.173388	-2.128421	1.956877	0.008617	0.700526
-45.830998	-2.164841	1.961882	0.008740	0.700214
-46.087597	-2.116914	1.966886	0.008787	0.700219
-46.676319	-2.016571	1.971891	0.008897	0.700210
-46.096380	-2.114248	1.976896	0.008789	0.700221
-45.983962	-2.139172	1.981901	0.008768	0.700211
-46.336052	-2.075178	1.986906	0.008834	0.700214
-45.944999	-2.171958	1.991910	0.008761	0.700159
-46.704384	-2.170678	1.996915	0.008902	0.699887
-47.233418	-2.073676	2.001920	0.009001	0.699892
-46.891345	-2.135120	2.011917	0.008937	0.699892
-47.164179	-2.086479	2.021914	0.008988	0.699892
-47.242743	-2.072561	2.031910	0.009002	0.699892
-46.949930	-2.125567	2.041907	0.008948	0.699890
-46.959515	-2.121794	2.051904	0.008949	0.699895
-46.976628	-2.170325	2.061901	0.008952	0.699790
-47.405504	-2.059196	2.071898	0.009032	0.699860
-46.969271	-2.122874	2.081894	0.008951	0.699889
-47.162550	-2.087420	2.091891	0.008987	0.699891
-46.843927	-2.143873	2.101888	0.008928	0.699892
-46.955350	-2.124903	2.111885	0.008948	0.699890
-47.146089	-2.090017	2.121882	0.008984	0.699892
-47.074832	-2.103434	2.131878	0.008970	0.699891
-47.120294	-2.073735	2.141875	0.008979	0.699935
-46.228692	-2.091521	2.151872	0.008813	0.700221
-46.061548	-2.122615	2.161869	0.008781	0.700219
-46.397145	-2.065558	2.171866	0.008844	0.700213
-46.115793	-2.115748	2.181862	0.008791	0.700213
-45.899260	-2.066472	2.191859	0.008751	0.700392
-45.276421	-2.109176	2.201856	0.008635	0.700530
-45.417168	-2.083784	2.211853	0.008661	0.700531
-45.481495	-2.073485	2.221850	0.008673	0.700529
-44.870503	-2.070254	2.231846	0.008559	0.700756
-44.660817	-2.051123	2.241843	0.008520	0.700871
-44.433441	-2.090605	2.251840	0.008478	0.700873
-44.354720	-2.106317	2.261837	0.008463	0.700870
-44.174935	-2.041142	2.271834	0.008430	0.701067
-43.757339	-2.091779	2.281830	0.008352	0.701116
-44.000622	-2.047216	2.291827	0.008397	0.701118
-43.495766	-2.063938	2.301824	0.008303	0.701267
-42.958199	-2.077135	2.311821	0.008203	0.701434
-43.043861	-2.062493	2.321818	0.008219	0.701433
-42.906008	-2.077594	2.331814	0.008193	0.701452
-42.216227	-2.058166	2.341811	0.008064	0.701741
-41.761517	-2.138684	2.351808	0.007980	0.701742
-41.877926	-2.117440	2.361805	0.008001	0.701743
-41.903191	-2.046863	2.371802	0.008006	0.701877
-40.897939	-2.130468	2.381798	0.007819	0.702070
-41.285935	-2.061686	2.391795	0.007891	0.702070
-40.852227	-2.137568	2.401792	0.007810	0.702073
-40.502303	-2.079476	2.411789	0.007745	0.702316
-40.417902	-2.069144	2.421786	0.007729	0.702368
-40.338722	-2.083858	2.431782	0.007714	0.702367
-40.154479	-2.050924	2.441779	0.007680	0.702500
-39.268055	-2.115294	2.451776	0.007515	0.702689
-39.457102	-2.080597	2.461773	0.007550	0.702691
-39.447513	-2.083715	2.471770	0.007548	0.702689
-38.819175	-2.041025	2.481766	0.007431	0.703001
-38.772080	-2.050134	2.491763	0.007422	0.703000
-38.363070	-2.120986	2.501760	0.007346	0.703004
-38.151696	-2.055476	2.511757	0.007307	0.703213
-37.469084	-2.116192	2.521754	0.007180	0.703336
-37.735276	-2.070064	2.531750	0.007229	0.703333
-37.478156	-2.115380	2.541747	0.007181	0.703335
-36.861860	-2.081892	2.551744	0.007066	0.703624
-36.858561	-2.080830	2.561741	0.007066	0.703627
-36.772947	-2.096652	2.571738	0.007050	0.703626
-36.750612	-2.005323	2.581734	0.007045	0.703819
-35.990027	-2.080462	2.591731	0.006904	0.703941
-35.913207	-2.092662	2.601728	0.006889	0.703944
-36.018569	-2.037662	2.611725	0.006909	0.704017
-34.998630	-2.103434	2.621722	0.006719	0.704251
-35.068072	-2.092310	2.631718	0.006732	0.704249
-34.953586	-2.112736	2.641715	0.006710	0.704249
-34.422238	-2.099269	2.651712	0.006611	0.704467
-34.243086	-2.075223	2.661709	0.006578	0.704580
-34.035047	-2.112599	2.671706	0.006539	0.704580
-34.356423	-2.034957	2.681702	0.006599	0.704621
-33.520546	-2.056745	2.691699	0.006443	0.704877
-33.431583	-2.070215	2.701696	0.006427	0.704882
-33.322700	-2.089875	2.711693	0.006406	0.704882
-32.914917	-2.033118	2.721690	0.006330	0.705143
-32.716229	-2.038082	2.731686	0.006293	0.705204
-32.278958	-2.115585	2.741683	0.006212	0.705205
-32.305480	-2.051199	2.751680	0.006217	0.705325
-31.540305	-2.089762	2.761677	0.006074	0.705522
-31.342169	-2.125254	2.771674	0.006037	0.705522
-31.614657	-2.078130	2.781670	0.006088	0.705519
-30.844451	-2.094559	2.791667	0.005944	0.705762
-30.741851	-2.065538	2.801664	0.005925	0.705858
-30.428475	-2.121573	2.811661	0.005867	0.705857
-30.602773	-2.079326	2.821658	0.005899	0.705880
-30.002925	-2.067067	2.831654	0.005788	0.706120
-29.739827	-2.113477	2.841651	0.005739	0.706121
-29.768900	-2.107416	2.851648	0.005744	0.706123
-29.311285	-2.092390	2.861645	0.005659	0.706317
-29.029630	-2.082802	2.871642	0.005606	0.706437
-29.336736	-2.028502	2.881638	0.005663	0.706437
-28.772589	-2.081162	2.891635	0.005558	0.706533
-28.075889	-2.099082	2.901632	0.005428	0.706746
-28.111264	-2.092286	2.911629	0.005435	0.706748
-28.392185	-2.043277	2.921626	0.005487	0.706746
-27.666781	-2.014354	2.931622	0.005352	0.707063
-27.314351	-2.073569	2.941619	0.005286	0.707071
-27.437305	-2.050617	2.951616	0.005309	0.707073
-26.617142	-2.097503	2.961613	0.005156	0.707272
-26.468359	-2.075321	2.971610	0.005129	0.707370
-26.609618	-2.049846	2.981606	0.005155	0.707371
-26.431980	-2.045965	2.991603	0.005122	0.707442
-25.890391	-2.015515	3.001600	0.005021	0.707697
-25.305302	-2.119506	3.011597	0.004912	0.707698
-25.593149	-2.069384	3.021594	0.004965	0.707696
-24.797966	-2.088840	3.031590	0.004817	0.707941
-24.715855	-2.069499	3.041587	0.004802	0.708009
-24.652627	-2.080433	3.051584	0.004790	0.708010
-24.561911	-2.062545	3.061581	0.004773	0.708078
-23.893996	-2.046296	3.071578	0.004649	0.708350
-23.791841	-2.067132	3.081574	0.004630	0.708344
-23.696326	-2.084444	3.091571	0.004612	0.708344
-23.272112	-2.061496	3.101568	0.004533	0.708541
-22.684458	-2.117791	3.111565	0.004423	0.708639
-23.173901	-2.030963	3.121562	0.004514	0.708638
-22.836203	-2.069822	3.131558	0.004451	0.708681
-22.143632	-2.058349	3.141555	0.004322	0.708951
-22.045551	-2.076196	3.151552	0.004304	0.708950
-22.242349	-2.039654	3.161549	0.004341	0.708953
-21.552162	-2.034846	3.171546	0.004212	0.709209
-21.343854	-2.047109	3.181542	0.004173	0.709259
-21.144953	-2.082925	3.191539	0.004136	0.709259
-21.064198	-2.031402	3.201536	0.004121	0.709391
-20.087589	-2.104281	3.211533	0.003939	0.709593
-20.413301	-2.046717	3.221530	0.004000	0.709592
-20.181382	-2.088690	3.231526	0.003956	0.709591
-19.826974	-2.028214	3.241523	0.003890	0.709838
-19.354708	-2.085579	3.251520	0.003802	0.709892
-19.328259	-2.091206	3.261517	0.003797	0.709890
-19.462494	-2.006038	3.271514	0.003822	0.710013
-18.500866	-2.077086	3.281510	0.003643	0.710214
-18.876628	-2.010293	3.291507	0.003713	0.710213
-18.414280	-2.090396	3.301504	0.003627	0.710218
-17.754865	-2.060604	3.311501	0.003504	0.710512
-17.857326	-2.031678	3.321498	0.003523	0.710534
-17.650405	-2.070289	3.331494	0.003485	0.710530
-17.724413	-1.980691	3.341491	0.003498	0.710683
-16.939429	-2.026965	3.351488	0.003352	0.710870
-16.950893	-2.020983	3.361485	0.003354	0.710878
-16.865991	-2.022700	3.371482	0.003338	0.710905
-16.279640	-2.010871	3.381478	0.003229	0.711137
-16.458012	-1.979570	3.391475	0.003262	0.711136
-16.198765	-2.024216	3.401472	0.003214	0.711140
-15.331901	-2.023347	3.411469	0.003052	0.711450
-15.049710	-2.070591	3.421466	0.003000	0.711456
-15.094995	-2.063281	3.431462	0.003008	0.711454
-15.003338	-2.030688	3.441459	0.002991	0.711552
-14.203388	-2.067701	3.451456	0.002842	0.711763
-14.266447	-2.056362	3.461453	0.002854	0.711763
-14.459373	-2.022392	3.471450	0.002890	0.711762
-13.521157	-2.045696	3.481446	0.002715	0.712049
-13.637594	-2.005630	3.491443	0.002737	0.712088
-13.193686	-2.084390	3.501440	0.002654	0.712088
-13.479996	-1.975656	3.511437	0.002707	0.712204
-12.442645	-2.070125	3.521434	0.002514	0.712384
-12.599011	-2.042553	3.531430	0.002543	0.712383
-12.593058	-2.044845	3.541427	0.002542	0.712381
-11.853823	-2.028984	3.551424	0.002404	0.712675
-11.707511	-2.036542	3.561421	0.002377	0.712712
-11.569948	-2.063188	3.571418	0.002351	0.712708
-11.494036	-2.016547	3.581414	0.002337	0.712828
-10.767583	-2.048148	3.591411	0.002202	0.713022
-10.661157	-2.066340	3.601408	0.002182	0.713024
-10.840060	-2.034243	3.611405	0.002215	0.713025
-9.945485	-2.060176	3.621402	0.002048	0.713290
-9.765922	-2.058945	3.631398	0.002015	0.713356
-9.486607	-2.108922	3.641395	0.001963	0.713356
-9.394944	-2.124011	3.651392	0.001946	0.713359
-8.987784	-2.084178	3.661389	0.001870	0.713582
-8.438863	-2.147953	3.671386	0.001768	0.713650
-8.421986	-2.150267	3.681382	0.001764	0.713652
-8.570615	-2.123802	3.691379	0.001792	0.713652
-7.949545	-2.118097	3.701376	0.001676	0.713883
-7.907071	-2.082541	3.711373	0.001668	0.713969
-7.548980	-2.145843	3.721370	0.001602	0.713970
-7.862750	-2.090506	3.731366	0.001660	0.713969
-6.894912	-2.109032	3.741363	0.001480	0.714275
-6.672529	-2.147093	3.751360	0.001438	0.714278
-6.721188	-2.138202	3.761357	0.001447	0.714279
-6.788764	-2.092340	3.771354	0.001460	0.714346
-5.891365	-2.120350	3.781350	0.001293	0.714608
-5.734550	-2.149208	3.791347	0.001263	0.714606
-5.713415	-2.152398	3.801344	0.001259	0.714607
-5.522491	-2.130289	3.811341	0.001224	0.714719
-4.636430	-2.193577	3.821338	0.001059	0.714907
-5.014596	-2.127718	3.831334	0.001129	0.714904
-4.731393	-2.177359	3.841331	0.001076	0.714905
-4.694861	-2.088606	3.851328	0.001069	0.715095
-3.859861	-2.169102	3.861325	0.000914	0.715230
-3.917888	-2.157715	3.871322	0.000925	0.715232
-3.846282	-2.172772	3.881318	0.000911	0.715228
-3.296966	-2.128067	3.891315	0.000809	0.715511
-3.197666	-2.130517	3.901312	0.000790	0.715541
-2.856372	-2.189361	3.911309	0.000727	0.715545
-2.898799	-2.142318	3.921306	0.000735	0.715623
-2.131800	-2.150031	3.931302	0.000592	0.715879
-1.831012	-2.203943	3.941299	0.000536	0.715878
-2.245216	-2.129226	3.951296	0.000613	0.715880
-1.759738	-2.157942	3.961293	0.000522	0.715995
-1.552833	-2.124873	3.971290	0.000484	0.716134
-1.401456	-2.153155	3.981286	0.000455	0.716131
-1.354682	-2.146313	3.991283	0.000447	0.716161
-1.214784	-2.026385	4.001280	0.000421	0.716448
-1.097862	-2.045925	4.011277	0.000399	0.716451
-1.020948	-2.011682	4.021274	0.000384	0.716546
-0.937788	-1.920464	4.031270	0.000369	0.716756
-0.836534	-1.938278	4.041267	0.000350	0.716756
-0.712506	-1.812359	4.051264	0.000327	0.717049
-0.772439	-1.783763	4.061261	0.000338	0.717085
-0.545841	-1.713351	4.071258	0.000295	0.717304
-0.555033	-1.672762	4.081254	0.000297	0.717381
-0.525366	-1.555247	4.091251	0.000291	0.717624
-0.615530	-1.496146	4.101248	0.000308	0.717709
-0.464047	-1.364474	4.111245	0.000280	0.718023
-0.368532	-1.320262	4.121242	0.000262	0.718144
-0.468702	-1.197498	4.131238	0.000280	0.718351
-0.532491	-1.059172	4.141235	0.000292	0.718602
-0.274440	-1.011745	4.151232	0.000244	0.718787
-0.330719	-0.898209	4.161229	0.000254	0.718991
-0.324938	-0.756232	4.171226	0.000253	0.719273
-0.191920	-0.647363	4.181222	0.000228	0.719535
-0.061730	-0.554002	4.191219	0.000204	0.719765
-0.071515	-0.426670	4.201216	0.000205	0.720012
0.037128	-0.306735	4.211213	0.000185	0.720287
0.175613	-0.195435	4.221210	0.000159	0.720554
0.127803	-0.022276	4.231206	0.000168	0.720879
0.201140	0.081590	4.241203	0.000154	0.721109
0.000000	0.275762	4.251200	0.000191	0.721420
0.332358	0.837653	4.256205	0.000129	0.722641
0.648831	2.055324	4.261210	0.000069	0.725137
0.529035	3.931065	4.266214	0.000090	0.728756
0.773182	6.292566	4.271219	0.000043	0.733422
1.260124	9.124163	4.276224	-0.000049	0.739045
1.525710	12.471279	4.281229	-0.000101	0.745531
1.770498	16.285272	4.286234	-0.000149	0.752835
2.140295	20.470735	4.291238	-0.000221	0.760803
2.628820	25.038583	4.296243	-0.000314	0.769432
3.149054	29.977939	4.301248	-0.000415	0.778652
3.568329	35.271335	4.306253	-0.000496	0.788370
4.020391	40.889365	4.311258	-0.000584	0.798556
4.321535	46.826342	4.316262	-0.000644	0.809126
5.018742	52.976586	4.321267	-0.000778	0.820049
5.655595	59.421756	4.326272	-0.000901	0.831314
6.337692	66.073411	4.331277	-0.001032	0.842789
6.776440	73.006697	4.336282	-0.001118	0.854505
7.321072	80.112106	4.341286	-0.001224	0.866375
7.520920	87.468499	4.346291	-0.001266	0.878392
9.224318	94.738291	4.351296	-0.001588	0.890529
13.092201	101.832740	4.356301	-0.002313	0.902824
13.701446	109.679693	4.361306	-0.002432	0.915232
14.119590	117.661431	4.366310	-0.002515	0.927628
14.725888	125.728152	4.371315	-0.002633	0.940039
15.973812	133.796155	4.376320	-0.002871	0.952456
16.955307	141.995493	4.381325	-0.003059	0.964837
17.509661	150.352828	4.386330	-0.003167	0.977182
19.118233	158.628982	4.391334	-0.003472	0.989520
19.653453	167.121808	4.396339	-0.003578	1.001747
20.914709	175.527454	4.401344	-0.003818	1.013880
21.899823	184.008422	4.406349	-0.004007	1.025908
23.010704	192.534449	4.411354	-0.004219	1.037886
23.416938	201.194697	4.416358	-0.004301	1.049744
24.372030	209.779801	4.421363	-0.004484	1.061496
25.951831	218.311946	4.426368	-0.004784	1.073191
26.620090	226.978738	4.431373	-0.004914	1.084729
27.359210	235.656435	4.436378	-0.005057	1.096175
28.160187	244.315743	4.441382	-0.005212	1.107493
29.156319	252.947776	4.446387	-0.005403	1.118704
29.823445	261.639777	4.451392	-0.005533	1.129807
30.867571	270.257428	4.456397	-0.005733	1.140790
32.171440	278.872908	4.461402	-0.005982	1.151720
33.123255	287.508605	4.466406	-0.006165	1.162497
33.824199	296.162466	4.471411	-0.006301	1.173146
34.694214	304.779073	4.476416	-0.006468	1.183687
34.860814	313.502972	4.481421	-0.006505	1.194121
35.430637	322.124638	4.486426	-0.006617	1.204424
36.619352	330.641957	4.491430	-0.006844	1.214641
37.596526	339.180378	4.496435	-0.007031	1.224755
38.439545	347.771368	4.501440	-0.007194	1.234820
39.093034	356.325136	4.506445	-0.007321	1.244724
39.765979	364.888317	4.511450	-0.007452	1.254564
40.462372	373.409890	4.516454	-0.007587	1.264284
41.318948	381.909465	4.521459	-0.007752	1.273936
41.930000	390.432956	4.526464	-0.007872	1.283496
42.395331	398.962115	4.531469	-0.007964	1.292964
43.112743	407.439272	4.536474	-0.008103	1.302352
43.441516	416.042017	4.541478	-0.008170	1.311738
44.172789	424.505928	4.546483	-0.008312	1.320981
44.826009	432.928918	4.551488	-0.008439	1.330101
45.469685	441.339168	4.556493	-0.008564	1.339144
45.995449	449.752917	4.561498	-0.008668	1.348110
46.622869	458.150070	4.566502	-0.008790	1.357015
47.150052	466.525521	4.571507	-0.008894	1.365823
48.132530	474.855642	4.576512	-0.009082	1.374606
48.891417	483.200207	4.581517	-0.009229	1.383309
49.495494	491.598339	4.586522	-0.009347	1.391986
50.226187	499.935045	4.591526	-0.009488	1.400567
51.059655	508.246471	4.596531	-0.009649	1.409088
51.825702	516.596440	4.601536	-0.009797	1.417585
52.395955	524.923190	4.606541	-0.009909	1.425975
52.931472	533.292020	4.611546	-0.010014	1.434352
53.518857	541.606844	4.616550	-0.010129	1.442636
53.850164	549.966622	4.621555	-0.010196	1.450875
54.634749	558.246404	4.626560	-0.010347	1.459062
55.092058	566.570170	4.631565	-0.010438	1.467193
55.375698	574.978233	4.636570	-0.010496	1.475333
55.930648	583.235753	4.641574	-0.010605	1.483327
56.859909	591.449285	4.646579	-0.010783	1.491294
57.735935	599.694742	4.651584	-0.010952	1.499241
57.869772	608.025533	4.656589	-0.010982	1.507111
58.534272	616.298276	4.661594	-0.011111	1.514967
59.078932	624.551140	4.666598	-0.011218	1.522746
59.478710	632.820582	4.671603	-0.011298	1.530479
60.347402	641.035759	4.676608	-0.011465	1.538192
60.800613	649.287766	4.681613	-0.011555	1.545839
61.155675	657.600919	4.686618	-0.011627	1.553490
61.681261	665.821460	4.691622	-0.011730	1.561043
62.238753	674.040357	4.696627	-0.011839	1.568564
62.902297	682.267195	4.701632	-0.011968	1.576070
63.407637	690.491876	4.706637	-0.012068	1.583516
64.024688	698.719876	4.711642	-0.012188	1.590947
64.461587	706.963580	4.716646	-0.012275	1.598330
64.837450	715.183200	4.721651	-0.012350	1.605650
65.288956	723.432062	4.726656	-0.012439	1.612972
65.721051	731.630108	4.731661	-0.012525	1.620214
66.091117	739.859153	4.736666	-0.012600	1.627442
66.826648	748.088664	4.741670	-0.012742	1.634689
67.390558	756.247754	4.746675	-0.012852	1.641820
68.056465	764.421639	4.751680	-0.012982	1.648946
68.293147	772.656897	4.756685	-0.013031	1.656035
68.708237	780.861073	4.761690	-0.013114	1.663091
69.380391	789.022401	4.766694	-0.013244	1.670116
69.565760	797.262216	4.771699	-0.013284	1.677112
70.261560	805.413515	4.776704	-0.013419	1.684073
70.685855	813.596219	4.781709	-0.013503	1.690995
71.052734	821.802173	4.786714	-0.013577	1.697901
71.271231	830.010117	4.791718	-0.013623	1.704760
71.680408	838.185871	4.796723	-0.013705	1.711591
72.332170	846.338762	4.801728	-0.013831	1.718406
72.683609	854.487487	4.806733	-0.013902	1.725153
73.168143	862.656398	4.811738	-0.013998	1.731906
73.732045	870.813847	4.816742	-0.014108	1.738634
74.098456	878.964381	4.821747	-0.014182	1.745305
74.391222	887.179077	4.826752	-0.014242	1.751993
74.887198	895.316195	4.831757	-0.014339	1.758619
75.582825	903.429057	4.836762	-0.014474	1.765225
76.019505	911.600675	4.841766	-0.014561	1.771821
76.454228	919.764492	4.846771	-0.014647	1.778386
77.093679	927.899767	4.851776	-0.014771	1.784929
77.429337	936.101634	4.856781	-0.014839	1.791464
78.078841	944.250073	4.861786	-0.014966	1.797971
78.565946	952.373045	4.866790	-0.015062	1.804414
78.887058	960.522458	4.871795	-0.015127	1.810835
79.498315	968.664753	4.876800	-0.015246	1.817263
79.763090	976.813295	4.881805	-0.015300	1.823631
80.439808	984.929986	4.886810	-0.015432	1.830001
80.770318	993.105585	4.891814	-0.015499	1.836353
81.079863	1001.243760	4.896819	-0.015562	1.842653
81.534150	1009.386877	4.901824	-0.015652	1.848951
81.963518	1017.529292	4.906829	-0.015737	1.855224
82.393746	1025.667330	4.911834	-0.015822	1.861473
82.862358	1033.796992	4.916838	-0.015915	1.867699
83.205318	1041.978373	4.921843	-0.015984	1.873929
84.033393	1050.036246	4.926848	-0.016144	1.880100
84.660750	1058.116347	4.931853	-0.016266	1.886245
85.101747	1066.272796	4.936858	-0.016353	1.892406
85.444558	1074.424041	4.941862	-0.016422	1.898531
85.678020	1082.555504	4.946867	-0.016471	1.904610
85.952949	1090.723967	4.951872	-0.016528	1.910701
86.313838	1098.852282	4.956877	-0.016600	1.916753
86.564232	1106.987264	4.961882	-0.016652	1.922778
86.897151	1115.108968	4.966886	-0.016719	1.928784
87.463817	1123.195695	4.971891	-0.016830	1.934771
88.049723	1131.297812	4.976896	-0.016945	1.940753
88.424923	1139.422329	4.981901	-0.017020	1.946710
89.025143	1147.564805	4.986906	-0.017137	1.952686
89.357419	1155.694492	4.991910	-0.017204	1.958605
89.600664	1163.793061	4.996915	-0.017255	1.964474
90.134343	1171.891797	5.001920	-0.017359	1.970357
90.720887	1179.972443	5.006925	-0.017474	1.976215
91.288722	1188.058068	5.011930	-0.017585	1.982057
91.650672	1196.177205	5.016934	-0.017658	1.987884
91.868860	1204.325585	5.021939	-0.017704	1.993699
92.387356	1212.420951	5.026944	-0.017805	1.999491
92.840087	1220.505088	5.031949	-0.017895	2.005252
93.184286	1228.639584	5.036954	-0.017965	2.011020
93.669538	1236.747291	5.041958	-0.018060	2.016767
93.934582	1244.850823	5.046963	-0.018115	2.022472
94.507723	1252.951277	5.051968	-0.018227	2.028191
94.848439	1261.098541	5.056973	-0.018296	2.033902
95.077020	1269.204269	5.061978	-0.018344	2.039557
95.711429	1277.264285	5.066982	-0.018467	2.045205
96.191379	1285.354610	5.071987	-0.018562	2.050844
96.602748	1293.482187	5.076992	-0.018644	2.056485
96.949373	1301.559774	5.081997	-0.018713	2.062070
97.205107	1309.671464	5.087002	-0.018766	2.067654
97.761611	1317.766681	5.092006	-0.018875	2.073242
97.937126	1325.876407	5.097011	-0.018913	2.078786
98.498488	1333.940298	5.102016	-0.019023	2.084323
98.754559	1342.051313	5.107021	-0.019076	2.089846
99.117611	1350.168019	5.112026	-0.019149	2.095370
99.765105	1358.213299	5.117030	-0.019275	2.100858
100.049510	1366.318740	5.122035	-0.019333	2.106338
100.292134	1374.482319	5.127040	-0.019384	2.111837
100.728739	1382.587291	5.132045	-0.019470	2.117302
101.087354	1390.648676	5.137050	-0.019542	2.122716
101.689723	1398.699371	5.142054	-0.019660	2.128133
102.105598	1406.793149	5.147059	-0.019742	2.133546
102.738249	1414.856169	5.152064	-0.019865	2.138946
103.078551	1422.941740	5.157069	-0.019934	2.144319
103.444306	1431.034735	5.162074	-0.020008	2.149686
104.005637	1439.118386	5.167078	-0.020117	2.155052
104.316153	1447.196206	5.172083	-0.020180	2.160377
104.678037	1455.291184	5.177088	-0.020253	2.165705
105.046745	1463.382410	5.182093	-0.020327	2.171018
105.726322	1471.445471	5.187098	-0.020459	2.176328
106.278272	1479.509548	5.192102	-0.020567	2.181614
106.378742	1487.636133	5.197107	-0.020591	2.186886
106.783429	1495.773460	5.202112	-0.020672	2.192180
106.973216	1503.861001	5.207117	-0.020712	2.197410
107.102995	1511.956016	5.212122	-0.020742	2.202627
107.551284	1520.016169	5.217126	-0.020831	2.207837
108.050459	1528.073885	5.222131	-0.020929	2.213039
108.445880	1536.164053	5.227136	-0.021008	2.218239
108.511341	1544.259467	5.232141	-0.021025	2.223401
108.923006	1552.326941	5.237146	-0.021107	2.228564
109.262894	1560.426194	5.242150	-0.021176	2.233729
109.449196	1568.506127	5.247155	-0.021216	2.238855
109.978997	1576.541419	5.252160	-0.021320	2.243973
110.392022	1584.605766	5.257165	-0.021402	2.249086
110.910548	1592.677321	5.262170	-0.021504	2.254202
111.344622	1600.757141	5.267174	-0.021590	2.259304
111.543301	1608.837488	5.272179	-0.021632	2.264373
112.014862	1616.925574	5.277184	-0.021725	2.269460
112.087089	1625.120067	5.282189	-0.021744	2.274568
112.296291	1633.154340	5.287194	-0.021788	2.279576
112.683620	1641.187399	5.292198	-0.021866	2.284588
112.700142	1649.286711	5.297203	-0.021874	2.289597
113.173793	1657.357582	5.302208	-0.021967	2.294618
113.591911	1665.377703	5.307213	-0.022051	2.299591
113.881182	1673.445635	5.312218	-0.022110	2.304572
114.215497	1681.529904	5.317222	-0.022177	2.309555
114.755110	1689.577978	5.322227	-0.022283	2.314523
114.986838	1697.656617	5.327232	-0.022331	2.319474
115.368087	1705.701492	5.332237	-0.022408	2.324405
115.821014	1713.761414	5.337242	-0.022497	2.329341
116.284890	1721.848343	5.342246	-0.022589	2.334284
116.713422	1729.875949	5.347251	-0.022674	2.339177
117.131357	1737.948239	5.352256	-0.022757	2.344087
117.292059	1746.059374	5.357261	-0.022792	2.348988
117.435618	1754.199504	5.362266	-0.022824	2.353895
117.744229	1762.249027	5.367270	-0.022887	2.358751
118.051317	1770.280860	5.372275	-0.022950	2.363586
118.468665	1778.345093	5.377280	-0.023033	2.368439
118.826838	1786.407394	5.382285	-0.023105	2.373276
119.233167	1794.472315	5.387290	-0.023186	2.378109
119.679148	1802.529665	5.392294	-0.023274	2.382931
119.724421	1810.629363	5.397299	-0.023288	2.387736
120.034885	1818.725804	5.402304	-0.023351	2.392550
120.533188	1826.748054	5.407309	-0.023449	2.397326
121.066116	1834.769560	5.412314	-0.023553	2.402095
121.645646	1842.825874	5.417318	-0.023666	2.406877
121.938440	1850.895988	5.422323	-0.023726	2.411636
122.107034	1859.020340	5.427328	-0.023763	2.416408
122.343413	1867.063144	5.432333	-0.023812	2.421128
122.863449	1875.089087	5.437338	-0.023914	2.425851
123.276586	1883.188618	5.442342	-0.023997	2.430599
123.671280	1891.295677	5.447347	-0.024075	2.435340
123.993554	1899.341330	5.452352	-0.024141	2.440031
124.299277	1907.343861	5.457357	-0.024203	2.444687
124.844029	1915.377778	5.462362	-0.024310	2.449370
124.987469	1923.499312	5.467366	-0.024342	2.454065
125.307241	1931.537391	5.472371	-0.024406	2.458715
125.746141	1939.585661	5.477376	-0.024493	2.463372
125.740090	1947.674580	5.482381	-0.024498	2.468009
125.994203	1955.751896	5.487386	-0.024550	2.472651
126.600737	1963.776251	5.492390	-0.024668	2.477280
126.536749	1971.853848	5.497395	-0.024662	2.481880
126.915713	1979.904007	5.502400	-0.024738	2.486490
127.157218	1987.968190	5.507405	-0.024788	2.491088
127.491124	1996.025283	5.512410	-0.024855	2.495681
127.717675	2004.106618	5.517414	-0.024903	2.500271
128.110086	2012.109921	5.522419	-0.024981	2.504821
128.671895	2020.161903	5.527424	-0.025091	2.509402
128.837568	2028.289910	5.532429	-0.025127	2.513989
129.137128	2036.313058	5.537434	-0.025188	2.518518
129.751046	2044.323905	5.542438	-0.025308	2.523054
129.974436	2052.368864	5.547443	-0.025355	2.527574
130.163861	2060.477450	5.552448	-0.025395	2.532118
130.599647	2068.516901	5.557453	-0.025482	2.536633
130.839236	2076.578564	5.562458	-0.025531	2.541139
131.187013	2084.609439	5.567462	-0.025601	2.545627
131.563438	2092.658956	5.572467	-0.025677	2.550119
132.018434	2100.741717	5.577472	-0.025767	2.554627
132.286344	2108.787851	5.582477	-0.025822	2.559094
132.367525	2116.841825	5.587482	-0.025842	2.563545
132.685017	2124.925105	5.592486	-0.025907	2.568020
133.020457	2132.959063	5.597491	-0.025975	2.572462
133.434845	2141.034461	5.602496	-0.026057	2.576924
133.528304	2149.102023	5.607501	-0.026080	2.581351
133.987094	2157.103959	5.612506	-0.026170	2.585761
134.090444	2165.204996	5.617510	-0.026195	2.590192
134.446646	2173.444808	5.622515	-0.026267	2.594709
134.907406	2181.396222	5.627520	-0.026358	2.599068
135.053613	2189.404810	5.632525	-0.026390	2.603430
135.070508	2197.464915	5.637530	-0.026399	2.607803
135.453209	2205.487899	5.642534	-0.026475	2.612173
135.732878	2213.512782	5.647539	-0.026532	2.616531
136.143787	2221.541612	5.652544	-0.026614	2.620891
136.435249	2229.580581	5.657549	-0.026674	2.625242
136.573496	2237.644156	5.662554	-0.026705	2.629589
136.795806	2245.732033	5.667558	-0.026751	2.633947
136.951910	2253.753307	5.672563	-0.026786	2.638258
137.678352	2261.733729	5.677568	-0.026926	2.642578
138.126015	2269.770640	5.682573	-0.027015	2.646902
138.188745	2277.864047	5.687578	-0.027032	2.651224
138.671062	2285.936669	5.692582	-0.027127	2.655555
138.927406	2293.941667	5.697587	-0.027180	2.659828
139.477852	2301.980325	5.702592	-0.027288	2.664132
139.690962	2310.054530	5.707597	-0.027333	2.668425
140.292382	2318.088167	5.712602	-0.027450	2.672715
140.724820	2326.152628	5.717606	-0.027536	2.677003
140.848403	2334.202555	5.722611	-0.027564	2.681257
141.342498	2342.222296	5.727616	-0.027661	2.685512
141.625033	2350.259217	5.732621	-0.027719	2.689756
142.029540	2358.335956	5.737626	-0.027800	2.694022
142.498558	2366.375648	5.742630	-0.027892	2.698265
142.860685	2374.389779	5.747635	-0.027965	2.702482
143.001367	2382.491062	5.752640	-0.027996	2.706723
143.133627	2390.554641	5.757645	-0.028026	2.710938
143.362444	2398.606107	5.762650	-0.028074	2.715146
143.646111	2406.656443	5.767654	-0.028132	2.719350
143.811848	2414.672694	5.772659	-0.028168	2.723522
144.207065	2422.731277	5.777664	-0.028247	2.727725
144.545562	2430.786328	5.782669	-0.028316	2.731915
144.772794	2438.841759	5.787674	-0.028363	2.736092
145.237925	2446.872984	5.792678	-0.028455	2.740265
145.827659	2454.861968	5.797683	-0.028570	2.744417
146.206829	2462.931982	5.802688	-0.028646	2.748592
146.116012	2471.088739	5.807693	-0.028634	2.752776
146.643293	2479.106553	5.812698	-0.028738	2.756921
147.071572	2487.116644	5.817702	-0.028823	2.761049
147.127742	2495.130678	5.822707	-0.028839	2.765150
147.592359	2503.151661	5.827712	-0.028930	2.769273
148.002237	2511.209652	5.832717	-0.029012	2.773406
148.195195	2519.259185	5.837722	-0.029053	2.777515
148.422733	2527.316726	5.842726	-0.029101	2.781624
148.728618	2535.329193	5.847731	-0.029163	2.785709
149.136238	2543.358433	5.852736	-0.029244	2.789802
149.170208	2551.476350	5.857741	-0.029256	2.793912
149.548607	2559.474887	5.862746	-0.029332	2.797976
150.043457	2567.503398	5.867750	-0.029429	2.802056
150.254213	2575.516508	5.872755	-0.029473	2.806106
150.421392	2583.603467	5.877760	-0.029510	2.810184
150.724185	2591.657459	5.882765	-0.029572	2.814247
150.958803	2599.698083	5.887770	-0.029620	2.818295
151.469258	2607.725669	5.892774	-0.029721	2.822345
151.555546	2615.783599	5.897779	-0.029742	2.826381
151.819451	2623.844086	5.902784	-0.029797	2.830422
152.076537	2631.917649	5.907789	-0.029850	2.834463
152.434099	2639.903636	5.912794	-0.029922	2.838461
152.979142	2647.895498	5.917798	-0.030028	2.842466
152.993261	2655.962906	5.922803	-0.030036	2.846474
153.371311	2663.989802	5.927808	-0.030112	2.850476
153.576417	2672.071706	5.932813	-0.030155	2.854490
153.997532	2680.081361	5.937818	-0.030239	2.858474
154.210226	2688.136018	5.942822	-0.030284	2.862464
154.481896	2696.174503	5.947827	-0.030340	2.866443
154.899918	2704.199647	5.952832	-0.030423	2.870419
155.151012	2712.263742	5.957837	-0.030475	2.874398
155.165035	2720.317316	5.962842	-0.030483	2.878354
155.778170	2728.323399	5.967846	-0.030602	2.882314
155.781100	2736.376286	5.972851	-0.030608	2.886258
156.270884	2744.422460	5.977856	-0.030704	2.890220
156.746957	2752.456525	5.982861	-0.030798	2.894170
156.907600	2760.502199	5.987866	-0.030833	2.898102
157.178833	2768.568469	5.992870	-0.030889	2.902046
157.405662	2776.589110	5.997875	-0.030937	2.905959
157.779943	2784.644956	6.002880	-0.031012	2.909892
157.822501	2792.798008	6.007885	-0.031025	2.913849
157.804390	2800.810834	6.012890	-0.031027	2.917730
158.237436	2808.806164	6.017894	-0.031113	2.921621
158.413079	2816.799183	6.022899	-0.031151	2.925492
158.611177	2824.836048	6.027904	-0.031193	2.929380
158.737092	2832.893523	6.032909	-0.031222	2.933269
159.159943	2840.893729	6.037914	-0.031306	2.937141
159.514237	2848.926479	6.042918	-0.031377	2.941020
159.706520	2856.944643	6.047923	-0.031418	2.944878
160.185999	2864.982091	6.052928	-0.031512	2.948755
160.394371	2873.040107	6.057933	-0.031556	2.952623
160.509457	2881.107763	6.062938	-0.031583	2.956486
160.972463	2889.098833	6.067942	-0.031675	2.960324
161.137956	2897.117444	6.072947	-0.031711	2.964156
161.471277	2905.184281	6.077952	-0.031778	2.968014
161.640895	2913.255686	6.082957	-0.031815	2.971861
161.819315	2921.293291	6.087962	-0.031853	2.975687
162.032295	2929.311308	6.092966	-0.031898	2.979501
162.167033	2937.348054	6.097971	-0.031929	2.983315
162.649064	2945.367477	6.102976	-0.032024	2.987133
162.854433	2953.411579	6.107981	-0.032067	2.990944
163.245624	2961.460273	6.112986	-0.032145	2.994762
163.736328	2969.475783	6.117990	-0.032242	2.998564
163.780226	2977.511725	6.122995	-0.032255	3.002348
163.805122	2985.572465	6.128000	-0.032265	3.006139
164.139639	2993.578233	6.133005	-0.032333	3.009914
164.263431	3001.639673	6.138010	-0.032361	3.013700
164.616895	3009.685256	6.143014	-0.032432	3.017485
164.791305	3017.708430	6.148019	-0.032470	3.021246
165.138728	3025.716951	6.153024	-0.032540	3.025004
165.305715	3033.769150	6.158029	-0.032576	3.028769
165.526384	3041.831913	6.163034	-0.032623	3.032537
166.054545	3049.864181	6.168038	-0.032726	3.036300
166.257405	3057.850338	6.173043	-0.032769	3.040022
166.399796	3065.912538	6.178048	-0.032801	3.043772
166.705375	3073.937596	6.183053	-0.032863	3.047507
166.887590	3081.991447	6.188058	-0.032902	3.051245
167.180448	3090.043225	6.193062	-0.032962	3.054983
167.274240	3098.060532	6.198067	-0.032985	3.058691
167.763891	3106.092438	6.203072	-0.033081	3.062420
167.998651	3114.129947	6.208077	-0.033130	3.066135
168.191454	3122.163966	6.213082	-0.033172	3.069842
168.536577	3130.283350	6.218086	-0.033241	3.073590
168.800174	3138.300690	6.223091	-0.033295	3.077284
168.923496	3146.331817	6.228096	-0.033324	3.080972
169.259186	3154.294526	6.233101	-0.033391	3.084635
169.782129	3162.294385	6.238106	-0.033494	3.088319
170.126288	3170.359708	6.243110	-0.033563	3.092020
170.237684	3178.411081	6.248115	-0.033589	3.095700
170.568038	3186.404866	6.253120	-0.033656	3.099359
170.734881	3194.472013	6.258125	-0.033692	3.103039
170.766373	3202.497118	6.263130	-0.033704	3.106690
171.095185	3210.538436	6.268134	-0.033770	3.110358
171.493206	3218.555666	6.273139	-0.033849	3.114013
171.600350	3226.624566	6.278144	-0.033875	3.117674
171.906848	3234.630071	6.283149	-0.033937	3.121311
172.415670	3242.592544	6.288154	-0.034037	3.124934
172.773234	3250.668035	6.293158	-0.034109	3.128596
172.768822	3258.711340	6.298163	-0.034113	3.132223
173.177869	3266.774549	6.303168	-0.034195	3.135874
173.436916	3274.796860	6.308173	-0.034248	3.139495
173.455845	3282.822249	6.313178	-0.034257	3.143103
173.888779	3290.871994	6.318182	-0.034343	3.146736
174.139390	3298.868276	6.323187	-0.034395	3.150332
174.735965	3306.931447	6.328192	-0.034511	3.153970
174.835046	3314.953514	6.333197	-0.034535	3.157563
175.298829	3322.973108	6.338202	-0.034626	3.161167
175.557618	3330.975780	6.343206	-0.034680	3.164750
175.588701	3339.027910	6.348211	-0.034691	3.168341
176.075782	3347.064100	6.353216	-0.034787	3.171941
176.246906	3355.109222	6.358221	-0.034824	3.175527
176.369377	3363.121809	6.363226	-0.034852	3.179092
176.716991	3371.165485	6.368230	-0.034922	3.182677
176.964441	3379.181499	6.373235	-0.034973	3.186241
177.245271	3387.237994	6.378240	-0.035031	3.189820
177.411862	3395.298341	6.383245	-0.035067	3.193392
177.622405	3403.316248	6.388250	-0.035112	3.196944
177.870554	3411.345979	6.393254	-0.035163	3.200498
177.839479	3419.324083	6.398259	-0.035163	3.204013
178.143115	3427.387804	6.403264	-0.035225	3.207577
178.648549	3435.427392	6.408269	-0.035324	3.211134
178.671117	3443.464777	6.413274	-0.035333	3.214666
178.883923	3451.505942	6.418278	-0.035378	3.218204
179.118758	3459.529774	6.423283	-0.035427	3.221731
179.413690	3467.520513	6.428288	-0.035487	3.225243
179.916606	3475.568517	6.433293	-0.035586	3.228784
179.841117	3483.664540	6.438298	-0.035578	3.232318
180.393084	3491.721736	6.443302	-0.035686	3.235857
180.408228	3499.679546	6.448307	-0.035694	3.239327
180.630714	3507.698412	6.453312	-0.035740	3.242829
180.908757	3515.738873	6.458317	-0.035797	3.246338
180.803522	3523.755981	6.463322	-0.035783	3.249817
181.065229	3531.837792	6.468326	-0.035837	3.253336
181.333031	3539.836443	6.473331	-0.035892	3.256815
181.553670	3547.851716	6.478336	-0.035938	3.260296
181.804618	3555.852682	6.483341	-0.035990	3.263768
182.077827	3563.897121	6.488346	-0.036047	3.267256
182.531925	3571.929473	6.493350	-0.036136	3.270742
182.749002	3579.970448	6.498355	-0.036182	3.274219
183.116153	3588.001391	6.503360	-0.036256	3.277693
183.514597	3596.028774	6.508365	-0.036335	3.281164
183.775641	3603.982089	6.513370	-0.036389	3.284593
184.070978	3612.066585	6.518374	-0.036449	3.288077
183.990354	3620.125179	6.523379	-0.036440	3.291531
184.401172	3628.153932	6.528384	-0.036521	3.294988
184.715181	3636.165699	6.533389	-0.036585	3.298430
184.732094	3644.190629	6.538394	-0.036593	3.301862
185.124829	3652.213813	6.543398	-0.036672	3.305305
185.168587	3660.263432	6.548403	-0.036685	3.308742
185.484139	3668.313440	6.553408	-0.036749	3.312186
185.909658	3676.340975	6.558413	-0.036834	3.315621
186.080070	3684.327641	6.563418	-0.036871	3.319025
186.310825	3692.360637	6.568422	-0.036919	3.322447
186.670967	3700.361955	6.573427	-0.036991	3.325858
186.770603	3708.393802	6.578432	-0.037015	3.329268
187.024713	3716.483073	6.583437	-0.037068	3.332705
187.399436	3724.498693	6.588442	-0.037143	3.336111
187.885189	3732.495279	6.593446	-0.037238	3.339510
187.935106	3740.518208	6.598451	-0.037253	3.342901
188.116079	3748.567547	6.603456	-0.037292	3.346304
188.709088	3756.575400	6.608461	-0.037408	3.349701
188.824658	3764.639615	6.613466	-0.037434	3.353100
189.258832	3772.671978	6.618470	-0.037520	3.356495
189.435189	3780.659051	6.623475	-0.037559	3.359858
189.814780	3788.679926	6.628480	-0.037635	3.363239
189.948227	3796.745038	6.633485	-0.037665	3.366626
189.982328	3804.754512	6.638490	-0.037676	3.369982
190.129159	3812.842986	6.643494	-0.037709	3.373373
190.464086	3820.843737	6.648499	-0.037776	3.376730
190.675916	3828.857081	6.653504	-0.037821	3.380085
190.909901	3836.884103	6.658509	-0.037870	3.383442
191.049943	3844.924905	6.663514	-0.037901	3.386799
191.135695	3852.986584	6.668518	-0.037923	3.390159
191.365929	3861.063681	6.673523	-0.037971	3.393528
191.704790	3869.074421	6.678528	-0.038039	3.396869
191.996097	3877.049047	6.683533	-0.038099	3.400190
192.250516	3885.020387	6.688538	-0.038151	3.403505
192.520359	3893.045829	6.693542	-0.038207	3.406840
192.771408	3901.070268	6.698547	-0.038259	3.410171
193.012093	3909.121662	6.703552	-0.038309	3.413509
193.412744	3917.143633	6.708557	-0.038389	3.416837
193.824300	3925.156073	6.713562	-0.038471	3.420158
194.029341	3933.188959	6.718566	-0.038514	3.423477
194.024091	3941.228821	6.723571	-0.038518	3.426789
194.246390	3949.252505	6.728576	-0.038565	3.430099
194.552804	3957.308323	6.733581	-0.038627	3.433421
194.668228	3965.361815	6.738586	-0.038654	3.436733
194.997245	3973.333447	6.743590	-0.038720	3.440015
195.182458	3981.346619	6.748595	-0.038760	3.443306
195.495387	3989.390005	6.753600	-0.038824	3.446611
195.875598	3997.398424	6.758605	-0.038900	3.449900
195.930989	4005.451541	6.763610	-0.038915	3.453194
196.294881	4013.522766	6.768614	-0.038988	3.456502
196.517730	4021.486888	6.773619	-0.039035	3.459759
196.666954	4029.538845	6.778624	-0.039068	3.463046
196.848355	4037.582155	6.783629	-0.039107	3.466327
197.025415	4045.574404	6.788634	-0.039145	3.469584
197.563441	4053.636273	6.793638	-0.039251	3.472878
197.712438	4061.674562	6.798643	-0.039284	3.476147
197.729783	4069.662369	6.803648	-0.039292	3.479388
197.983554	4077.683702	6.808653	-0.039345	3.482647
198.173299	4085.678367	6.813658	-0.039385	3.485890
198.424319	4093.729814	6.818662	-0.039437	3.489155
198.579210	4101.760896	6.823667	-0.039472	3.492406
198.794342	4109.773950	6.828672	-0.039517	3.495648
199.037871	4117.806278	6.833677	-0.039568	3.498896
199.266964	4125.797708	6.838682	-0.039615	3.502123
199.588582	4133.836000	6.843686	-0.039681	3.505370
199.903999	4141.845886	6.848691	-0.039745	3.508602
199.932812	4149.918040	6.853696	-0.039755	3.511847
200.170171	4157.965313	6.858701	-0.039805	3.515085
200.443633	4165.959736	6.863706	-0.039861	3.518301
200.732870	4174.009498	6.868710	-0.039920	3.521536
200.970826	4181.968526	6.873715	-0.039969	3.524730
201.189528	4190.024582	6.878720	-0.040015	3.527959
201.383559	4198.078277	6.883725	-0.040057	3.531184
201.429993	4206.123227	6.888730	-0.040071	3.534398
201.634411	4214.176908	6.893734	-0.040114	3.537617
201.890944	4222.169058	6.898739	-0.040167	3.540810
202.070904	4230.186064	6.903744	-0.040206	3.544008
202.351599	4238.209919	6.908749	-0.040263	3.547209
202.564356	4246.205373	6.913754	-0.040308	3.550393
202.606951	4254.370226	6.918758	-0.040322	3.553637
202.821986	4262.369943	6.923763	-0.040367	3.556817
203.121213	4270.297406	6.928768	-0.040428	3.559968
203.324055	4278.333798	6.933773	-0.040471	3.563157
203.247425	4286.370475	6.938778	-0.040462	3.566335
203.605023	4294.361019	6.943782	-0.040534	3.569505
203.949808	4302.419872	6.948787	-0.040603	3.572698
204.139652	4310.445991	6.953792	-0.040644	3.575871
204.115781	4318.457696	6.958797	-0.040644	3.579029
204.260168	4326.469778	6.963802	-0.040677	3.582189
204.697154	4334.473325	6.968806	-0.040763	3.585352
204.641793	4342.488808	6.973811	-0.040758	3.588502
205.069446	4350.539249	6.978816	-0.040843	3.591677
205.516441	4358.557429	6.983821	-0.040932	3.594837
205.534639	4366.574641	6.988826	-0.040940	3.597982
205.857806	4374.589797	6.993830	-0.041006	3.601132
205.970319	4382.568929	6.998835	-0.041032	3.604259
206.324553	4390.604107	7.003840	-0.041103	3.607412
206.296028	4398.672869	7.008845	-0.041103	3.610565
206.630652	4406.678161	7.013850	-0.041171	3.613700
206.870842	4414.754876	7.018854	-0.041221	3.616857
206.944396	4422.746335	7.023859	-0.041240	3.619974
207.250705	4430.734786	7.028864	-0.041302	3.623094
207.798617	4438.767926	7.033869	-0.041409	3.626235
207.983089	4446.760564	7.038874	-0.041449	3.629347
208.294439	4454.862280	7.043878	-0.041512	3.632502
208.577524	4462.899110	7.048883	-0.041570	3.635629
208.672654	4470.912516	7.053888	-0.041593	3.638739
208.742640	4478.961169	7.058893	-0.041611	3.641859
208.759656	4486.915517	7.063898	-0.041620	3.644938
209.190537	4494.964469	7.068902	-0.041705	3.648063
209.302458	4502.985789	7.073907	-0.041731	3.651166
209.671291	4511.022330	7.078912	-0.041805	3.654278
210.218686	4519.061023	7.083917	-0.041912	3.657394
210.370185	4527.047000	7.088922	-0.041946	3.660476
210.796651	4535.069825	7.093926	-0.042030	3.663576
211.191634	4543.101772	7.098931	-0.042109	3.666677
211.390814	4551.121385	7.103936	-0.042152	3.669766
211.508647	4559.193966	7.108941	-0.042179	3.672869
211.705064	4567.209583	7.113946	-0.042221	3.675951
211.997618	4575.206057	7.118950	-0.042280	3.679025
212.015433	4583.246385	7.123955	-0.042289	3.682106
212.065586	4591.212996	7.128960	-0.042303	3.685157
212.304035	4599.270950	7.133965	-0.042353	3.688245
212.521629	4607.302823	7.138970	-0.042399	3.691320
212.728902	4615.330726	7.143974	-0.042443	3.694391
212.835257	4623.351560	7.148979	-0.042468	3.697454
213.252506	4631.331740	7.153984	-0.042551	3.700507
213.302055	4639.392684	7.158989	-0.042565	3.703579
213.562736	4647.404777	7.163994	-0.042619	3.706635
213.968873	4655.427323	7.168998	-0.042700	3.709695
214.140290	4663.497325	7.174003	-0.042737	3.712766
214.160845	4671.563237	7.179008	-0.042746	3.715829
214.350446	4679.527811	7.184013	-0.042787	3.718854
214.605373	4687.533511	7.189018	-0.042839	3.721895
214.646410	4695.496022	7.194022	-0.042852	3.724911
214.704446	4703.564629	7.199027	-0.042868	3.727966
215.017022	4711.574178	7.204032	-0.042932	3.731002
215.115612	4719.620461	7.209037	-0.042956	3.734044
215.459082	4727.635580	7.214042	-0.043025	3.737078
215.909745	4735.653948	7.219046	-0.043114	3.740112
216.043768	4743.651629	7.224051	-0.043144	3.743130
215.954304	4751.698815	7.229056	-0.043133	3.746158
216.139082	4759.738728	7.234061	-0.043172	3.749187
216.452969	4767.763097	7.239066	-0.043236	3.752211
216.732283	4775.821999	7.244070	-0.043293	3.755244
216.772667	4783.814074	7.249075	-0.043306	3.758245
216.832513	4791.829687	7.254080	-0.043323	3.761252
217.047224	4799.850593	7.259085	-0.043368	3.764263
217.144505	4807.866843	7.264090	-0.043391	3.767267
217.644924	4815.905901	7.269094	-0.043490	3.770286
217.733655	4823.932334	7.274099	-0.043511	3.773288
218.063604	4831.978207	7.279104	-0.043578	3.776301
218.489379	4839.966299	7.284109	-0.043663	3.779292
218.583769	4847.985019	7.289114	-0.043685	3.782284
218.653646	4855.986461	7.294118	-0.043704	3.785267
218.787597	4864.019785	7.299123	-0.043734	3.788261
219.143253	4872.056408	7.304128	-0.043805	3.791259
219.445475	4880.142214	7.309133	-0.043867	3.794271
219.643328	4888.107060	7.314138	-0.043909	3.797234
219.914327	4896.101679	7.319142	-0.043965	3.800207
220.045009	4904.088188	7.324147	-0.043994	3.803172
220.119738	4912.117982	7.329152	-0.044013	3.806149
220.443784	4920.151363	7.334157	-0.044079	3.809131
220.919109	4928.151998	7.339162	-0.044173	3.812101
221.106755	4936.203642	7.344166	-0.044213	3.815081
221.180789	4944.252170	7.349171	-0.044232	3.818056
221.651678	4952.202934	7.354176	-0.044325	3.821001
221.936207	4960.224086	7.359181	-0.044383	3.823965
221.846217	4968.249278	7.364186	-0.044372	3.826921
222.128829	4976.331502	7.369190	-0.044430	3.829903
222.337763	4984.319087	7.374195	-0.044474	3.832846
222.625176	4992.361984	7.379200	-0.044533	3.835809
222.888413	5000.351387	7.384205	-0.044587	3.838750
223.146305	5008.385623	7.389210	-0.044640	3.841705
223.186740	5016.385553	7.394214	-0.044653	3.844640
223.153455	5024.422152	7.399219	-0.044652	3.847585
223.423794	5032.455687	7.404224	-0.044707	3.850533
223.627092	5040.488978	7.409229	-0.044751	3.853477
223.774079	5048.540158	7.414234	-0.044783	3.856424
224.220536	5056.517836	7.419238	-0.044872	3.859348
224.341024	5064.542736	7.424243	-0.044899	3.862280
224.299644	5072.556959	7.429248	-0.044897	3.865204
224.743327	5080.608223	7.434253	-0.044985	3.868148
224.942516	5088.632789	7.439258	-0.045027	3.871075
225.102604	5096.900730	7.444262	-0.045062	3.874088
225.191066	5104.824411	7.449267	-0.045084	3.876971
225.617078	5112.699828	7.454272	-0.045168	3.879842
225.829677	5120.762950	7.459277	-0.045213	3.882775
225.820583	5128.721873	7.464282	-0.045217	3.885663
226.246611	5136.735103	7.469286	-0.045301	3.888577
226.359052	5144.776293	7.474291	-0.045328	3.891493
226.565466	5152.809992	7.479296	-0.045371	3.894406
226.794108	5160.855541	7.484301	-0.045419	3.897321
227.164931	5168.795256	7.489306	-0.045493	3.900198
227.452999	5176.853374	7.494310	-0.045552	3.903115
227.365854	5184.851482	7.499315	-0.045541	3.906001
227.679599	5192.856383	7.504320	-0.045605	3.908894
227.903242	5200.937849	7.509325	-0.045652	3.911811
227.711596	5208.949656	7.514330	-0.045622	3.914694
228.085914	5216.968719	7.519334	-0.045696	3.917587
228.279465	5224.950116	7.524339	-0.045738	3.920461
228.609849	5232.953979	7.529344	-0.045804	3.923343
228.806426	5241.006297	7.534349	-0.045846	3.926239
229.105631	5248.981155	7.539354	-0.045907	3.929106
229.300303	5257.083924	7.544358	-0.045949	3.932015
229.404311	5265.071804	7.549363	-0.045973	3.934879
229.526856	5273.062889	7.554368	-0.046002	3.937743
229.878879	5281.089497	7.559373	-0.046072	3.940621
230.047394	5289.045588	7.564378	-0.046109	3.943468
230.533288	5297.102914	7.569382	-0.046205	3.946356
230.729280	5305.142943	7.574387	-0.046246	3.949229
230.851297	5313.224921	7.579392	-0.046274	3.952115
230.788306	5321.283309	7.584397	-0.046268	3.954986
231.209175	5329.228547	7.589402	-0.046352	3.957824
231.533841	5337.219406	7.594406	-0.046417	3.960674
231.615735	5345.200605	7.599411	-0.046438	3.963514
231.645235	5353.226100	7.604416	-0.046448	3.966368
231.895208	5361.284702	7.609421	-0.046500	3.969234
232.047460	5369.291404	7.614426	-0.046534	3.972079
232.344118	5377.357854	7.619430	-0.046594	3.974945
232.449850	5385.384607	7.624435	-0.046619	3.977791
232.583864	5393.369983	7.629440	-0.046650	3.980622
232.857209	5401.367842	7.634445	-0.046706	3.983457
232.857455	5409.390392	7.639450	-0.046711	3.986294
233.238733	5417.434617	7.644454	-0.046787	3.989143
233.392581	5425.464287	7.649459	-0.046821	3.991982
233.425580	5433.507944	7.654464	-0.046833	3.994821
233.823048	5441.537152	7.659469	-0.046912	3.997659
234.016386	5449.489356	7.664474	-0.046953	4.000464
234.090774	5457.549287	7.669478	-0.046972	4.003303
234.134568	5465.570209	7.674483	-0.046986	4.006127
234.439167	5473.568229	7.679488	-0.047048	4.008944
234.471032	5481.658861	7.684493	-0.047059	4.011788
234.764158	5489.619109	7.689498	-0.047119	4.014587
235.277882	5497.689191	7.694502	-0.047220	4.017427
235.431350	5505.677785	7.699507	-0.047253	4.020231
235.452750	5513.689416	7.704512	-0.047263	4.023038
235.811777	5521.728463	7.709517	-0.047335	4.025859
236.107580	5529.732323	7.714522	-0.047395	4.028664
236.334079	5537.776159	7.719526	-0.047442	4.031480
236.510415	5545.900285	7.724531	-0.047481	4.034321
236.515202	5553.875694	7.729536	-0.047487	4.037106
236.699758	5561.822081	7.734541	-0.047526	4.039881
236.864072	5569.833097	7.739546	-0.047562	4.042677
237.205533	5577.823407	7.744550	-0.047631	4.045466
237.321611	5585.858486	7.749555	-0.047658	4.048266
237.423911	5593.847703	7.754560	-0.047682	4.051047
237.702246	5601.932108	7.759565	-0.047739	4.053862
238.168910	5609.914657	7.764570	-0.047831	4.056643
238.393606	5617.904807	7.769574	-0.047878	4.059421
238.445864	5625.962537	7.774579	-0.047893	4.062217
238.531719	5633.927199	7.779584	-0.047915	4.064980
238.793119	5641.992004	7.784589	-0.047969	4.067778
238.772428	5649.993667	7.789594	-0.047970	4.070549
239.225066	5658.031287	7.794598	-0.048060	4.073337
239.210563	5666.046435	7.799603	-0.048062	4.076108
239.259238	5674.034687	7.804608	-0.048076	4.078869
239.693691	5682.073605	7.809613	-0.048163	4.081651
239.730868	5690.046159	7.814618	-0.048175	4.084403
240.054704	5698.109706	7.819622	-0.048240	4.087188
240.026614	5706.129272	7.824627	-0.048240	4.089951
240.265270	5714.172858	7.829632	-0.048290	4.092725
240.484160	5722.197366	7.834637	-0.048336	4.095489
240.522368	5730.189884	7.839642	-0.048348	4.098238
240.934092	5738.217949	7.844646	-0.048430	4.101003
241.123416	5746.231933	7.849651	-0.048471	4.103758
241.166742	5754.244209	7.854656	-0.048484	4.106508
241.419931	5762.319492	7.859661	-0.048537	4.109281
241.554012	5770.308246	7.864666	-0.048567	4.112021
241.826826	5778.375603	7.869670	-0.048623	4.114788
242.060163	5786.366954	7.874675	-0.048672	4.117526
242.446078	5794.328851	7.879680	-0.048749	4.120254
242.683057	5802.394880	7.884685	-0.048798	4.123015
242.505416	5810.380160	7.889690	-0.048770	4.125740
242.767029	5818.369251	7.894694	-0.048824	4.128471
243.042174	5826.421844	7.899699	-0.048881	4.131221
242.977200	5834.462900	7.904704	-0.048874	4.133961
243.318806	5842.516662	7.909709	-0.048943	4.136709
243.454526	5850.478713	7.914714	-0.048973	4.139422
243.524030	5858.511740	7.919718	-0.048991	4.142156
243.947785	5866.508194	7.924723	-0.049076	4.144880
244.093311	5874.550204	7.929728	-0.049108	4.147614
244.300805	5882.582545	7.934733	-0.049152	4.150344
244.428494	5890.600953	7.939738	-0.049181	4.153066
244.765706	5898.637701	7.944742	-0.049249	4.155796
245.061667	5906.618630	7.949747	-0.049309	4.158504
244.974350	5914.658567	7.954752	-0.049298	4.161225
245.037465	5922.668175	7.959757	-0.049315	4.163937
245.224028	5930.654857	7.964762	-0.049355	4.166640
245.376373	5938.695083	7.969766	-0.049389	4.169359
245.453110	5946.742230	7.974771	-0.049408	4.172078
245.785812	5954.727877	7.979776	-0.049476	4.174778
245.795345	5962.791534	7.984781	-0.049483	4.177498
245.880241	5970.745890	7.989786	-0.049504	4.180180
246.156310	5978.789080	7.994790	-0.049560	4.182893
246.571994	5986.778354	7.999795	-0.049643	4.185587
246.615764	5994.821144	8.004800	-0.049656	4.188294
246.808319	6002.869968	8.009805	-0.049698	4.191002
246.895814	6010.927431	8.014810	-0.049719	4.193710
246.927905	6018.976089	8.019814	-0.049730	4.196413
247.027390	6026.886380	8.024819	-0.049754	4.199069
247.321093	6034.966070	8.029824	-0.049814	4.201782
247.589246	6042.898150	8.034829	-0.049869	4.204443
247.586612	6050.920191	8.039834	-0.049874	4.207130
247.739473	6058.902476	8.044838	-0.049908	4.209803
247.871163	6066.990449	8.049843	-0.049937	4.212510
248.191915	6074.999483	8.054848	-0.050002	4.215190
248.322638	6083.004515	8.059853	-0.050032	4.217866
248.461736	6090.989184	8.064858	-0.050063	4.220533
248.736339	6099.009576	8.069862	-0.050120	4.223212
248.879640	6107.043737	8.074867	-0.050151	4.225892
248.970894	6115.022734	8.079872	-0.050174	4.228552
249.250594	6123.068834	8.084877	-0.050231	4.231234
249.427070	6131.130655	8.089882	-0.050269	4.233918
249.579505	6139.174887	8.094886	-0.050303	4.236595
249.761625	6147.136045	8.099891	-0.050342	4.239243
249.920107	6155.151823	8.104896	-0.050377	4.241907
250.254811	6163.171514	8.109901	-0.050444	4.244572
250.152395	6171.184132	8.114906	-0.050430	4.247229
250.317549	6179.231986	8.119910	-0.050467	4.249899
250.360814	6187.254402	8.124915	-0.050480	4.252557
250.608450	6195.269668	8.129920	-0.050531	4.255214
250.909135	6203.293327	8.134925	-0.050592	4.257871
250.924004	6211.284510	8.139930	-0.050600	4.260514
251.175875	6219.302670	8.144934	-0.050653	4.263166
251.278310	6227.358272	8.149939	-0.050677	4.265828
251.592592	6235.359433	8.154944	-0.050741	4.268471
251.683188	6243.421727	8.159949	-0.050763	4.271132
251.868681	6251.422205	8.164954	-0.050803	4.273771
252.054014	6259.476060	8.169958	-0.050842	4.276426
252.034995	6267.418826	8.174963	-0.050844	4.279041
252.327526	6275.459136	8.179968	-0.050904	4.281689
252.541452	6283.472343	8.184973	-0.050949	4.284326
252.585424	6291.487233	8.189978	-0.050962	4.286960
252.632378	6299.510807	8.194982	-0.050976	4.289596
253.023695	6307.546081	8.199987	-0.051054	4.292236
253.310606	6315.552844	8.204992	-0.051113	4.294865
253.539492	6323.566043	8.209997	-0.051161	4.297494
253.638464	6331.533039	8.215002	-0.051185	4.300104
253.819479	6339.607886	8.220006	-0.051224	4.302750
253.865622	6347.601262	8.225011	-0.051237	4.305366
254.083338	6355.639427	8.230016	-0.051283	4.307996
254.406218	6363.646708	8.235021	-0.051349	4.310615
254.328004	6371.705545	8.240026	-0.051339	4.313247
254.610067	6379.742856	8.245030	-0.051397	4.315872
254.871234	6387.687052	8.250035	-0.051451	4.318466
254.999132	6395.690861	8.255040	-0.051480	4.321076
255.318953	6403.696247	8.260045	-0.051545	4.323687
255.457750	6411.692387	8.265050	-0.051576	4.326292
255.880027	6419.766851	8.270054	-0.051660	4.328922
255.880875	6427.796980	8.275059	-0.051665	4.331534
256.007852	6435.779285	8.280064	-0.051694	4.334129
256.306149	6443.871421	8.285069	-0.051755	4.336760
256.463775	6451.802256	8.290074	-0.051790	4.339335
256.646921	6459.859588	8.295078	-0.051829	4.341951
257.018617	6467.812000	8.300083	-0.051903	4.344532
257.100414	6475.865846	8.305088	-0.051924	4.347142
257.267015	6483.874631	8.310093	-0.051960	4.349737
257.257105	6491.954550	8.315098	-0.051964	4.352352
257.636798	6500.024797	8.320102	-0.052040	4.354964
257.594713	6507.993424	8.325107	-0.052037	4.357540
257.641232	6515.954388	8.330112	-0.052051	4.360112
258.073842	6524.018027	8.335117	-0.052137	4.362718
258.172230	6531.927584	8.340122	-0.052160	4.365271
258.252100	6539.985490	8.345126	-0.052180	4.367870
258.551744	6548.007284	8.350131	-0.052241	4.370458
258.727892	6556.035286	8.355136	-0.052279	4.373044
259.043170	6564.088844	8.360141	-0.052343	4.375639
259.074055	6572.047656	8.365146	-0.052354	4.378200
259.315210	6580.073407	8.370150	-0.052405	4.380781
259.399073	6588.128181	8.375155	-0.052425	4.383370
259.440552	6596.062088	8.380160	-0.052438	4.385918
259.760289	6604.143680	8.385165	-0.052503	4.388514
260.013255	6612.140800	8.390170	-0.052556	4.391081
260.151121	6620.215782	8.395174	-0.052586	4.393670
260.463080	6628.206882	8.400179	-0.052650	4.396232
260.548067	6636.135355	8.405184	-0.052671	4.398771
260.742874	6644.199363	8.410189	-0.052712	4.401353
260.981733	6652.192288	8.415194	-0.052762	4.403910
261.412147	6660.247463	8.420198	-0.052848	4.406487
261.413316	6668.260573	8.425203	-0.052853	4.409047
261.469202	6676.292164	8.430208	-0.052869	4.411611
261.856762	6684.360518	8.435213	-0.052946	4.414187
262.151457	6692.381304	8.440218	-0.053006	4.416747
262.550231	6700.381779	8.445222	-0.053086	4.419298
262.511991	6708.426888	8.450227	-0.053084	4.421860
262.866419	6716.372780	8.455232	-0.053155	4.424391
263.131966	6724.435582	8.460237	-0.053210	4.426958
263.001867	6732.438117	8.465242	-0.053191	4.429502
263.414089	6740.488661	8.470246	-0.053273	4.432062
263.692359	6748.539013	8.475251	-0.053330	4.434619
263.709671	6756.558353	8.480256	-0.053338	4.437165
263.800094	6764.505519	8.485261	-0.053360	4.439686
263.894416	6772.521222	8.490266	-0.053383	4.442228
264.366166	6780.517876	8.495270	-0.053476	4.444763
264.369688	6788.577619	8.500275	-0.053482	4.447316
264.590246	6796.567201	8.505280	-0.053529	4.449845
264.730498	6804.626608	8.510285	-0.053560	4.452395
264.858670	6812.596998	8.515290	-0.053589	4.454915
264.932728	6820.638844	8.520294	-0.053608	4.457456
265.138532	6828.637256	8.525299	-0.053652	4.459982
265.242886	6836.638517	8.530304	-0.053676	4.462508
265.561942	6844.623060	8.535309	-0.053741	4.465027
265.646993	6852.675345	8.540314	-0.053762	4.467566
265.773481	6860.685197	8.545318	-0.053791	4.470089
265.890677	6868.737426	8.550323	-0.053818	4.472625
266.136633	6876.731359	8.555328	-0.053869	4.475141
266.489004	6884.778417	8.560333	-0.053940	4.477673
266.544588	6892.723975	8.565338	-0.053955	4.480171
266.670914	6900.757773	8.570343	-0.053984	4.482695
266.875873	6908.750609	8.575347	-0.054028	4.485205
267.060103	6916.775086	8.580352	-0.054067	4.487724
267.390652	6924.806725	8.585357	-0.054134	4.490244
267.606101	6932.849082	8.590362	-0.054179	4.492765
267.549135	6940.877631	8.595367	-0.054174	4.495280
267.554618	6948.901118	8.600371	-0.054180	4.497792
267.896995	6956.824319	8.605376	-0.054249	4.500272
268.215169	6964.896042	8.610381	-0.054314	4.502797
268.113793	6972.881056	8.615386	-0.054300	4.505292
268.269291	6980.963317	8.620391	-0.054334	4.507817
268.695064	6988.936966	8.625395	-0.054419	4.510308
268.768253	6997.025064	8.630400	-0.054438	4.512832
268.898400	7005.052197	8.635405	-0.054467	4.515335
269.200296	7013.014425	8.640410	-0.054529	4.517817
269.273930	7020.982821	8.645415	-0.054548	4.520300
269.232685	7029.055755	8.650419	-0.054545	4.522813
269.758690	7036.977706	8.655424	-0.054648	4.525279
269.927694	7045.041150	8.660429	-0.054685	4.527787
270.068986	7053.027932	8.665434	-0.054717	4.530269
270.135280	7061.079952	8.670439	-0.054734	4.532771
270.494447	7069.153773	8.675443	-0.054807	4.535278
270.453785	7077.150038	8.680448	-0.054804	4.537759
270.421475	7085.125449	8.685453	-0.054803	4.540232
270.606748	7093.136241	8.690458	-0.054843	4.542716
270.738684	7101.131619	8.695463	-0.054873	4.545193
270.844480	7109.147691	8.700467	-0.054898	4.547675
270.929710	7117.141045	8.705472	-0.054919	4.550148
271.220436	7125.278169	8.710477	-0.054979	4.552665
271.227279	7133.264613	8.715482	-0.054985	4.555134
271.412217	7141.251590	8.720487	-0.055025	4.557601
271.649634	7149.259950	8.725491	-0.055074	4.560074
271.820106	7157.293264	8.730496	-0.055111	4.562553
272.106266	7165.274895	8.735501	-0.055170	4.565015
272.108257	7173.300471	8.740506	-0.055175	4.567489
272.381449	7181.289954	8.745511	-0.055231	4.569951
272.582167	7189.364214	8.750515	-0.055274	4.572437
272.645443	7197.365232	8.755520	-0.055291	4.574900
272.877562	7205.412761	8.760525	-0.055340	4.577375
272.932474	7213.370734	8.765530	-0.055355	4.579822
273.064387	7221.432412	8.770535	-0.055385	4.582299
273.244261	7229.413997	8.775539	-0.055424	4.584750
273.575666	7237.433202	8.780544	-0.055491	4.587211
273.567573	7245.488016	8.785549	-0.055494	4.589682
273.921588	7253.506856	8.790554	-0.055565	4.592140
274.339075	7261.535144	8.795559	-0.055648	4.594601
274.361410	7269.586753	8.800563	-0.055658	4.597066
274.482875	7277.467111	8.805568	-0.055686	4.599478
274.860842	7285.596436	8.810573	-0.055761	4.601965
274.903815	7293.515026	8.815578	-0.055775	4.604386
275.066935	7301.582863	8.820583	-0.055810	4.606852
275.242071	7309.578406	8.825587	-0.055848	4.609294
275.405302	7317.584404	8.830592	-0.055884	4.611738
275.626860	7325.625433	8.835597	-0.055930	4.614191
275.836652	7333.659568	8.840602	-0.055975	4.616641
276.097062	7341.640704	8.845607	-0.056028	4.619073
276.171548	7349.694715	8.850611	-0.056047	4.621527
276.377128	7357.652635	8.855616	-0.056091	4.623949
276.711016	7365.703219	8.860621	-0.056158	4.626399
276.642170	7373.727909	8.865626	-0.056151	4.628839
276.778242	7381.731435	8.870631	-0.056181	4.631272
276.915572	7389.787545	8.875635	-0.056212	4.633719
276.959696	7397.773749	8.880640	-0.056226	4.636144
277.198898	7405.803666	8.885645	-0.056276	4.638581
277.243800	7413.814817	8.890650	-0.056289	4.641011
277.523279	7421.744237	8.895655	-0.056346	4.643414
277.770894	7429.788077	8.900659	-0.056398	4.645851
277.504923	7437.785286	8.905664	-0.056353	4.648273
277.821976	7445.885326	8.910669	-0.056418	4.650725
278.202021	7453.877457	8.915674	-0.056494	4.653142
278.294759	7461.866715	8.920679	-0.056516	4.655558
278.397714	7469.945974	8.925683	-0.056541	4.657999
278.413438	7477.910285	8.930688	-0.056549	4.660405
278.643173	7485.912687	8.935693	-0.056597	4.662820
278.764821	7493.898180	8.940698	-0.056625	4.665229
278.957858	7501.981369	8.945703	-0.056666	4.667667
279.001589	7509.997725	8.950707	-0.056679	4.670083
279.021536	7518.012960	8.955712	-0.056688	4.672497
279.513741	7526.108352	8.960717	-0.056785	4.674934
279.462557	7534.124408	8.965722	-0.056781	4.677346
279.635361	7542.045086	8.970727	-0.056818	4.679728
279.642660	7550.051014	8.975731	-0.056825	4.682135
279.874366	7557.977142	8.980736	-0.056873	4.684516
280.186139	7566.096091	8.985741	-0.056937	4.686954
280.298126	7574.042338	8.990746	-0.056963	4.689339
280.726108	7582.073799	8.995751	-0.057048	4.691748
280.889736	7590.153655	9.000755	-0.057084	4.694170
280.894225	7598.161658	9.005760	-0.057090	4.696570
281.006819	7606.151579	9.010765	-0.057116	4.698963
281.101324	7614.174702	9.015770	-0.057139	4.701365
281.369757	7622.161502	9.020775	-0.057194	4.703754
281.407359	7630.192504	9.025779	-0.057206	4.706156
281.573022	7638.222351	9.030784	-0.057242	4.708556
281.921975	7646.257817	9.035789	-0.057313	4.710955
281.968032	7654.245916	9.040794	-0.057326	4.713341
282.020353	7662.277898	9.045799	-0.057341	4.715738
282.187847	7670.256351	9.050803	-0.057378	4.718117
282.205375	7678.236553	9.055808	-0.057386	4.720497
282.310811	7686.325320	9.060813	-0.057411	4.722907
282.652595	7694.268388	9.065818	-0.057480	4.725272
282.791432	7702.387824	9.070823	-0.057511	4.727688
282.888880	7710.393537	9.075827	-0.057535	4.730070
283.120231	7718.390974	9.080832	-0.057583	4.732448
283.379627	7726.414869	9.085837	-0.057636	4.734832
283.363507	7734.420174	9.090842	-0.057639	4.737210
283.322238	7742.417678	9.095847	-0.057636	4.739585
283.609245	7750.494163	9.100851	-0.057695	4.741982
283.697859	7758.404305	9.105856	-0.057717	4.744328
283.667131	7766.474045	9.110861	-0.057716	4.746720
283.828343	7774.458291	9.115866	-0.057751	4.749086
284.138348	7782.506244	9.120871	-0.057814	4.751469
284.126455	7790.613760	9.125875	-0.057818	4.753869
284.288282	7798.526873	9.130880	-0.057853	4.756210
284.551180	7806.538066	9.135885	-0.057907	4.758578
284.627091	7814.574356	9.140890	-0.057926	4.760953
284.900064	7822.551568	9.145895	-0.057983	4.763309
284.918941	7830.587856	9.150899	-0.057991	4.765682
284.917346	7838.575005	9.155904	-0.057996	4.768040
285.226982	7846.653718	9.160909	-0.058059	4.770422
285.536704	7854.640220	9.165914	-0.058122	4.772775
285.746351	7862.641128	9.170919	-0.058166	4.775133
285.950791	7870.714918	9.175923	-0.058210	4.777510
285.860824	7878.650935	9.180928	-0.058198	4.779847
286.201109	7886.723011	9.185933	-0.058267	4.782221
286.278368	7894.651170	9.190938	-0.058286	4.784552
286.483728	7902.753946	9.195943	-0.058330	4.786933
286.690527	7910.707820	9.200947	-0.058374	4.789270
286.661974	7918.762196	9.205952	-0.058374	4.791635
286.824548	7926.791450	9.210957	-0.058409	4.793991
286.934957	7934.844168	9.215962	-0.058435	4.796353
287.185459	7942.766717	9.220967	-0.058487	4.798676
287.344466	7950.827114	9.225971	-0.058522	4.801037
287.448226	7958.773438	9.230976	-0.058546	4.803365
287.629154	7966.850719	9.235981	-0.058585	4.805729
287.896042	7974.822453	9.240986	-0.058640	4.808061
288.042039	7982.879488	9.245991	-0.058673	4.810417
288.262147	7990.406653	9.250995	-0.058719	4.812617
288.232869	7995.067722	9.256000	-0.058716	4.813979
288.368162	7997.597822	9.261005	-0.058743	4.814718
288.398113	7998.869883	9.266010	-0.058749	4.815089
288.519373	7999.675482	9.271015	-0.058773	4.815324
288.643854	7999.680746	9.276019	-0.058796	4.815325
288.741906	7999.684504	9.281024	-0.058814	4.815326
288.965310	7999.682851	9.286029	-0.058856	4.815324
288.964885	7999.977797	9.291034	-0.058856	4.815410
289.077869	7999.996765	9.296039	-0.058877	4.815415
289.228883	7999.973613	9.301043	-0.058905	4.815408
289.285046	8000.118816	9.306048	-0.058916	4.815450
289.438418	7999.871281	9.311053	-0.058944	4.815377
289.408656	8000.142237	9.316058	-0.058939	4.815456
289.415307	7999.882659	9.321063	-0.058940	4.815380
289.666476	8000.077037	9.326067	-0.058987	4.815436
289.849072	7999.952882	9.331072	-0.059021	4.815399
289.720128	7999.855642	9.336077	-0.058997	4.815371
289.544921	7999.974580	9.341082	-0.058964	4.815407
289.604790	7999.981983	9.346087	-0.058975	4.815409
289.865591	7999.856983	9.351091	-0.059024	4.815371
289.848853	8000.119608	9.356096	-0.059021	4.815448
289.961237	7999.838264	9.361101	-0.059042	4.815365
290.015769	7999.970616	9.366106	-0.059052	4.815403
290.110280	7999.900578	9.371111	-0.059070	4.815382
290.159483	7999.991164	9.376115	-0.059079	4.815409
289.971960	7999.983793	9.381120	-0.059044	4.815407
290.113603	7999.965830	9.386125	-0.059070	4.815401
290.114839	7999.965853	9.391130	-0.059071	4.815401
290.195178	7999.977871	9.396135	-0.059086	4.815404
290.330283	7999.844381	9.401139	-0.059111	4.815365
290.311606	7999.972319	9.406144	-0.059107	4.815402
290.251358	7999.971326	9.411149	-0.059096	4.815402
290.164045	8000.128054	9.416154	-0.059080	4.815449
290.388014	7999.972520	9.421159	-0.059122	4.815402
290.454075	7999.849645	9.426163	-0.059134	4.815366
290.341497	7999.949314	9.431168	-0.059113	4.815395
290.634267	7999.957361	9.436173	-0.059168	4.815396
290.485668	7999.974144	9.441178	-0.059140	4.815402
290.540634	7999.982536	9.446183	-0.059150	4.815404
290.433066	7999.878165	9.451187	-0.059130	4.815374
290.432813	8000.138929	9.456192	-0.059130	4.815450
290.576477	7999.850616	9.461197	-0.059157	4.815365
290.537329	7999.966461	9.466202	-0.059150	4.815399
290.433283	7999.858942	9.471207	-0.059130	4.815369
290.557648	7999.837488	9.476211	-0.059153	4.815362
290.420868	7999.973093	9.481216	-0.059128	4.815402
290.705490	7999.861311	9.486221	-0.059181	4.815368
290.674859	7999.819127	9.491226	-0.059175	4.815356
290.556301	7999.875950	9.496231	-0.059153	4.815373
290.808095	7999.959198	9.501235	-0.059200	4.815396
290.812770	8000.069356	9.506240	-0.059201	4.815428
290.704858	7999.868794	9.511245	-0.059181	4.815370
290.542440	8000.061686	9.516250	-0.059151	4.815427
290.674113	7999.980505	9.521255	-0.059175	4.815403
290.908924	8000.005763	9.526259	-0.059219	4.815409
290.656316	8000.120218	9.531264	-0.059172	4.815444
290.726364	7999.996338	9.536269	-0.059185	4.815407
290.982382	8000.017672	9.541274	-0.059233	4.815412
290.700592	8000.071796	9.546279	-0.059181	4.815429
290.929021	7999.914198	9.551283	-0.059223	4.815382
290.852722	8000.090347	9.556288	-0.059209	4.815434
290.829965	7999.879436	9.561293	-0.059205	4.815373
290.812684	8000.147401	9.566298	-0.059202	4.815451
290.836427	7999.944739	9.571303	-0.059206	4.815392
290.881026	7999.943342	9.576307	-0.059214	4.815391
290.902467	7999.934080	9.581312	-0.059218	4.815388
290.936487	8000.110984	9.586317	-0.059225	4.815440
290.970409	8000.091242	9.591322	-0.059231	4.815434
291.038981	7999.902145	9.596327	-0.059244	4.815378
291.067937	7999.834229	9.601331	-0.059249	4.815358
291.126043	7999.911070	9.606336	-0.059260	4.815380
291.154070	7999.921155	9.611341	-0.059265	4.815383
291.008054	7999.986073	9.616346	-0.059238	4.815403
291.187417	7999.894993	9.621351	-0.059272	4.815375
291.392992	7999.882363	9.626355	-0.059310	4.815371
291.010621	8000.005360	9.631360	-0.059239	4.815409
291.087980	7999.843127	9.636365	-0.059253	4.815361
291.072514	7999.951883	9.641370	-0.059250	4.815393
291.103180	7999.844452	9.646375	-0.059256	4.815361
290.930743	7999.958095	9.651379	-0.059224	4.815395
291.019682	8000.125220	9.656384	-0.059241	4.815444
291.000492	7999.928260	9.661389	-0.059237	4.815386
291.036746	8000.058177	9.666394	-0.059244	4.815424
291.128997	7999.982756	9.671399	-0.059261	4.815401
291.379218	7999.953765	9.676403	-0.059308	4.815392
291.397632	7999.948728	9.681408	-0.059311	4.815390
291.352709	7999.925545	9.686413	-0.059303	4.815384
291.345992	7999.997041	9.691418	-0.059302	4.815404
291.243088	7999.922669	9.696423	-0.059282	4.815383
291.290988	7999.898883	9.701427	-0.059291	4.815376
291.202949	7999.941248	9.706432	-0.059275	4.815389
291.312277	7999.762444	9.711437	-0.059295	4.815336
291.125689	7999.944250	9.716442	-0.059261	4.815390
291.169603	7999.846657	9.721447	-0.059269	4.815361
291.159448	7999.965119	9.726451	-0.059267	4.815396
291.187146	7999.979473	9.731456	-0.059272	4.815400
291.343572	7999.854883	9.736461	-0.059301	4.815363
291.284432	7999.978949	9.741466	-0.059290	4.815399
291.316382	7999.998717	9.746471	-0.059296	4.815405
291.308669	7999.800878	9.751475	-0.059295	4.815347
291.323281	7999.991355	9.756480	-0.059298	4.815403
291.527673	7999.852595	9.761485	-0.059336	4.815361
291.313152	7999.983711	9.766490	-0.059296	4.815401
291.321379	8000.089654	9.771495	-0.059297	4.815432
291.586383	7999.998921	9.776499	-0.059347	4.815404
291.404065	7999.829188	9.781504	-0.059313	4.815355
291.352945	7999.974761	9.786509	-0.059303	4.815398
291.286578	7999.962979	9.791514	-0.059291	4.815395
291.385011	7999.865217	9.796519	-0.059309	4.815366
291.393148	7999.839705	9.801523	-0.059311	4.815358
291.205958	7999.939210	9.806528	-0.059276	4.815388
291.416997	7999.847585	9.811533	-0.059315	4.815360
291.447985	7999.850237	9.816538	-0.059321	4.815361
291.456175	8000.094046	9.821543	-0.059323	4.815432
291.617031	8000.013347	9.826547	-0.059353	4.815408
291.712452	8000.065158	9.831552	-0.059371	4.815423
291.501954	7999.915263	9.836557	-0.059331	4.815380
291.554218	8000.126671	9.841562	-0.059341	4.815441
291.685491	8000.002733	9.846567	-0.059366	4.815404
291.745318	7999.864789	9.851571	-0.059377	4.815364
291.689658	8000.004944	9.856576	-0.059366	4.815405
291.646617	7999.750946	9.861581	-0.059358	4.815331
291.642124	7999.853472	9.866586	-0.059358	4.815361
291.435129	7999.952650	9.871591	-0.059319	4.815391
291.622661	7999.847811	9.876595	-0.059354	4.815360
291.556568	7999.989931	9.881600	-0.059342	4.815401
291.606144	7999.838994	9.886605	-0.059351	4.815357
291.492294	7999.972843	9.891610	-0.059330	4.815397
291.745993	7999.953528	9.896615	-0.059377	4.815390
291.684199	7999.832810	9.901619	-0.059366	4.815355
291.528741	7999.990553	9.906624	-0.059337	4.815402
291.674152	7999.756770	9.911629	-0.059364	4.815333
291.607726	7999.971558	9.916634	-0.059352	4.815396
291.471832	7999.891296	9.921639	-0.059326	4.815373
291.583698	7999.952997	9.926643	-0.059347	4.815390
291.717381	7999.971241	9.931648	-0.059372	4.815395
291.807746	7999.835939	9.936653	-0.059389	4.815355
291.817092	7999.981445	9.941658	-0.059391	4.815398
291.674552	8000.003671	9.946663	-0.059364	4.815405
291.706895	7999.993521	9.951667	-0.059370	4.815402
291.560834	8000.011414	9.956672	-0.059343	4.815408
291.833315	7999.955004	9.961677	-0.059394	4.815390
291.884291	7999.965469	9.966682	-0.059403	4.815393
291.839357	7999.870679	9.971687	-0.059395	4.815365
291.842389	7999.844013	9.976691	-0.059395	4.815357
291.819019	7999.987909	9.981696	-0.059391	4.815399
291.818634	7999.844694	9.986701	-0.059391	4.815358
291.835229	7999.962532	9.991706	-0.059394	4.815392
291.815452	7999.955795	9.996711	-0.059391	4.815390
291.922500	7999.889169	10.001715	-0.059411	4.815370
291.830228	7999.860927	10.006720	-0.059393	4.815362
291.905777	7999.856835	10.011725	-0.059407	4.815361
292.029749	7999.850337	10.016730	-0.059431	4.815358
292.006783	7999.856373	10.021735	-0.059426	4.815360
292.003576	7999.860597	10.026739	-0.059426	4.815361
291.949750	7999.851160	10.031744	-0.059416	4.815359
291.925512	7999.883892	10.036749	-0.059411	4.815369
291.777291	7999.852588	10.041754	-0.059384	4.815360
291.933201	7999.957768	10.046759	-0.059413	4.815390
291.976022	7999.850536	10.051763	-0.059421	4.815359
291.864765	7999.976947	10.056768	-0.059400	4.815396
291.960886	7999.986020	10.061773	-0.059418	4.815398
291.925420	7999.970474	10.066778	-0.059412	4.815394
291.973433	7999.974477	10.071783	-0.059420	4.815395
292.088621	7999.842791	10.076787	-0.059442	4.815356
291.936939	7999.977085	10.081792	-0.059414	4.815396
292.056438	7999.938451	10.086797	-0.059436	4.815384
291.943059	8000.004978	10.091802	-0.059415	4.815404
292.102965	7999.859070	10.096807	-0.059445	4.815360
292.078420	7999.927066	10.101811	-0.059440	4.815380
291.924762	8000.004683	10.106816	-0.059412	4.815404
292.017877	7999.876908	10.111821	-0.059429	4.815366
292.102393	8000.102745	10.116826	-0.059445	4.815432
292.106102	7999.875165	10.121831	-0.059445	4.815365
292.037842	7999.843046	10.126835	-0.059433	4.815356
291.970607	8000.124085	10.131840	-0.059420	4.815439
291.952124	7999.964538	10.136845	-0.059417	4.815392
291.838128	8000.012887	10.141850	-0.059396	4.815407
291.835936	7999.884604	10.146855	-0.059395	4.815369
291.933763	7999.840269	10.151859	-0.059413	4.815356
291.876588	7999.979331	10.156864	-0.059403	4.815397
291.885125	7999.944206	10.161869	-0.059405	4.815386
291.857702	8000.041011	10.166874	-0.059400	4.815415
291.913202	8000.001319	10.171879	-0.059410	4.815403
292.066990	7999.986764	10.176883	-0.059439	4.815398
291.972944	8000.001243	10.181888	-0.059421	4.815403
292.246866	7999.899969	10.186893	-0.059472	4.815372
291.955623	7999.967830	10.191898	-0.059418	4.815393
291.913417	7999.961791	10.196903	-0.059410	4.815391
291.954445	7999.887660	10.201907	-0.059418	4.815370
292.022409	8000.067267	10.206912	-0.059430	4.815422
292.027114	7999.869630	10.211917	-0.059431	4.815364
292.090675	7999.899539	10.216922	-0.059443	4.815372
291.996323	7999.911875	10.221927	-0.059426	4.815376
292.023853	7999.869583	10.226931	-0.059431	4.815364
291.932150	7999.993112	10.231936	-0.059414	4.815400
292.036104	7999.845210	10.236941	-0.059433	4.815357
292.085310	7999.949694	10.241946	-0.059442	4.815387
292.067190	8000.038103	10.246951	-0.059439	4.815413
292.057105	7999.904345	10.251955	-0.059437	4.815374
291.981372	8000.173489	10.256960	-0.059423	4.815453
292.124792	7999.969595	10.261965	-0.059450	4.815393
292.348413	7999.980777	10.266970	-0.059491	4.815395
292.110498	7999.999288	10.271975	-0.059447	4.815401
292.155434	7999.849341	10.276979	-0.059455	4.815357
292.190861	7999.953597	10.281984	-0.059462	4.815388
292.142992	7999.858759	10.286989	-0.059453	4.815360
292.152237	7999.868533	10.291994	-0.059455	4.815363
292.034087	7999.943531	10.296999	-0.059433	4.815385
292.192028	7999.857439	10.302003	-0.059462	4.815360
292.218795	8000.093010	10.307008	-0.059468	4.815428
292.240906	8000.012153	10.312013	-0.059472	4.815404
292.419749	7999.972363	10.317018	-0.059505	4.815392
292.356256	8000.007653	10.322023	-0.059493	4.815403
292.467713	7999.879111	10.327027	-0.059514	4.815365
292.221000	7999.836559	10.332032	-0.059468	4.815353
292.454239	7999.869274	10.337037	-0.059511	4.815362
292.511734	7999.865953	10.342042	-0.059522	4.815360
292.198227	8000.007189	10.347047	-0.059464	4.815403
292.466823	7999.788265	10.352051	-0.059514	4.815338
292.297750	8000.040903	10.357056	-0.059483	4.815413
292.285356	7999.855807	10.362061	-0.059480	4.815359
292.487084	7999.999152	10.367066	-0.059518	4.815399
292.463362	7999.884406	10.372071	-0.059513	4.815366
292.584886	7999.963368	10.377075	-0.059536	4.815389
292.622839	7999.989649	10.382080	-0.059543	4.815396
292.560536	7999.819758	10.387085	-0.059531	4.815347
292.418255	7999.895426	10.392090	-0.059505	4.815370
292.272332	7999.971034	10.397095	-0.059478	4.815392
292.458566	7999.997629	10.402099	-0.059513	4.815399
292.545747	8000.105951	10.407104	-0.059529	4.815430
292.539123	7999.858960	10.412109	-0.059528	4.815358
292.631457	7999.976984	10.417114	-0.059545	4.815392
292.601721	7999.993595	10.422119	-0.059539	4.815397
292.581617	7999.855395	10.427123	-0.059536	4.815357
292.275415	7999.967896	10.432128	-0.059479	4.815391
292.355061	7999.863410	10.437133	-0.059494	4.815360
292.324135	8000.025351	10.442138	-0.059488	4.815408
292.428935	8000.017468	10.447143	-0.059507	4.815405
292.502754	7999.916091	10.452147	-0.059521	4.815375
292.358437	7999.997070	10.457152	-0.059494	4.815399
292.401925	7999.864197	10.462157	-0.059502	4.815360
292.463616	7999.972096	10.467162	-0.059514	4.815392
292.514083	7999.993239	10.472167	-0.059523	4.815398
292.529566	8000.002048	10.477171	-0.059526	4.815400
292.367244	7999.987609	10.482176	-0.059496	4.815397
292.578245	7999.884226	10.487181	-0.059535	4.815365
292.474919	7999.968020	10.492186	-0.059516	4.815390
292.345646	7999.972297	10.497191	-0.059492	4.815392
292.312829	7999.843507	10.502195	-0.059486	4.815355
292.304186	7999.964135	10.507200	-0.059485	4.815390
292.435372	7999.857294	10.512205	-0.059509	4.815358
292.490491	7999.844315	10.517210	-0.059519	4.815354
292.386375	7999.981533	10.522215	-0.059500	4.815395
292.520320	7999.872601	10.527219	-0.059525	4.815362
292.320077	8000.003954	10.532224	-0.059488	4.815402
292.361143	7999.889211	10.537229	-0.059495	4.815368
292.545251	7999.939283	10.542234	-0.059530	4.815382
292.276877	7999.962635	10.547239	-0.059480	4.815390
292.564171	7999.955633	10.552243	-0.059533	4.815386
292.634780	7999.948253	10.557248	-0.059546	4.815384
292.492274	7999.878567	10.562253	-0.059520	4.815364
292.340349	8000.037439	10.567258	-0.059492	4.815411
292.495461	7999.951300	10.572263	-0.059521	4.815385
292.582764	7999.942059	10.577267	-0.059537	4.815382
292.318930	8000.068086	10.582272	-0.059488	4.815420
292.553460	8000.053799	10.587277	-0.059531	4.815415
292.600102	8000.007548	10.592282	-0.059540	4.815401
292.422799	7999.984311	10.597287	-0.059507	4.815395
292.587911	7999.990251	10.602291	-0.059538	4.815396
292.511545	7999.983647	10.607296	-0.059524	4.815395
292.655156	7999.859911	10.612301	-0.059550	4.815358
292.470904	7999.861141	10.617306	-0.059516	4.815359
292.481769	7999.969268	10.622311	-0.059518	4.815391
292.810581	7999.859283	10.627315	-0.059579	4.815357
292.370659	7999.987741	10.632320	-0.059498	4.815397
292.514825	7999.870428	10.637325	-0.059524	4.815362
292.674080	8000.000247	10.642330	-0.059554	4.815399
292.634153	7999.852100	10.647335	-0.059547	4.815356
292.632167	7999.852070	10.652339	-0.059546	4.815356
292.446811	7999.989014	10.657344	-0.059512	4.815397
292.441187	7999.965410	10.662349	-0.059511	4.815390
292.354124	7999.953285	10.667354	-0.059495	4.815387
292.670729	7999.992725	10.672359	-0.059554	4.815397
292.673997	7999.838880	10.677363	-0.059554	4.815352
292.670899	7999.864482	10.682368	-0.059554	4.815359
292.676087	7999.880601	10.687373	-0.059555	4.815364
292.720555	7999.871721	10.692378	-0.059563	4.815361
292.492992	7999.986591	10.697383	-0.059521	4.815396
292.675955	7999.877401	10.702387	-0.059555	4.815363
292.838443	7999.854440	10.707392	-0.059585	4.815355
292.775437	7999.967758	10.712397	-0.059573	4.815389
292.673514	7999.897674	10.717402	-0.059554	4.815369
292.526225	7999.996773	10.722407	-0.059527	4.815399
292.718885	7999.864229	10.727411	-0.059563	4.815359
292.537395	8000.094220	10.732416	-0.059529	4.815427
292.647991	7999.882299	10.737421	-0.059550	4.815365
292.688001	7999.747232	10.742426	-0.059557	4.815325
292.666858	7999.868723	10.747431	-0.059553	4.815360
292.619316	7999.875420	10.752435	-0.059545	4.815363
292.577754	7999.969855	10.757440	-0.059537	4.815390
292.610313	7999.852833	10.762445	-0.059543	4.815356
292.742694	7999.861437	10.767450	-0.059568	4.815358
292.630940	7999.980361	10.772455	-0.059547	4.815393
292.625742	7999.857370	10.777459	-0.059546	4.815357
292.510575	7999.948450	10.782464	-0.059525	4.815385
292.625505	7999.875540	10.787469	-0.059546	4.815363
292.571593	7999.980458	10.792474	-0.059536	4.815394
292.818914	7999.979208	10.797479	-0.059582	4.815392
293.060786	7999.858166	10.802483	-0.059627	4.815355
292.935424	7999.860370	10.807488	-0.059604	4.815357
292.911721	7999.994645	10.812493	-0.059599	4.815396
292.785685	7999.837592	10.817498	-0.059576	4.815351
292.846758	8000.002125	10.822503	-0.059587	4.815399
292.877570	7999.853011	10.827507	-0.059593	4.815355
292.642249	7999.864084	10.832512	-0.059549	4.815359
292.677750	7999.774898	10.837517	-0.059556	4.815333
292.802381	7999.969338	10.842522	-0.059579	4.815389
292.726464	7999.924266	10.847527	-0.059565	4.815376
292.874937	7999.923518	10.852531	-0.059593	4.815375
292.937170	7999.846530	10.857536	-0.059604	4.815353
292.821609	7999.862790	10.862541	-0.059583	4.815358
292.723967	7999.954160	10.867546	-0.059565	4.815385
292.706379	7999.823483	10.872551	-0.059561	4.815347
292.880589	7999.909730	10.877555	-0.059594	4.815371
292.706336	8000.085334	10.882560	-0.059562	4.815424
292.892140	7999.898170	10.887565	-0.059596	4.815368
292.854788	8000.024738	10.892570	-0.059589	4.815405
292.667339	7999.891250	10.897575	-0.059554	4.815367
292.703679	7999.832003	10.902579	-0.059561	4.815350
292.581629	7999.958238	10.907584	-0.059538	4.815387
292.569392	7999.900325	10.912589	-0.059536	4.815370
292.580497	7999.955018	10.917594	-0.059538	4.815386
292.706444	7999.870535	10.922599	-0.059562	4.815361
292.899879	7999.928244	10.927603	-0.059598	4.815377
292.708767	8000.070437	10.932608	-0.059562	4.815419
292.624934	7999.981414	10.937613	-0.059547	4.815394
292.863446	7999.982155	10.942618	-0.059591	4.815393
292.748877	7999.984538	10.947623	-0.059570	4.815394
292.756823	7999.961159	10.952627	-0.059571	4.815387
292.801505	8000.040989	10.957632	-0.059580	4.815410
292.940326	7999.871217	10.962637	-0.059606	4.815360
292.703680	7999.856618	10.967642	-0.059561	4.815357
292.712558	7999.971124	10.972647	-0.059563	4.815390
292.869642	7999.867918	10.977651	-0.059592	4.815359
292.639123	7999.944264	10.982656	-0.059550	4.815383
292.869760	7999.949151	10.987661	-0.059593	4.815383
292.824501	7999.887485	10.992666	-0.059584	4.815365
292.881723	7999.962179	10.997671	-0.059595	4.815387
292.703211	7999.752958	11.002675	-0.059562	4.815326
292.636590	7999.836291	11.007680	-0.059549	4.815351
292.962300	7999.991308	11.012685	-0.059610	4.815395
292.901494	7999.857777	11.017690	-0.059599	4.815356
292.719996	7999.865465	11.022695	-0.059565	4.815359
292.667671	7999.883840	11.027699	-0.059555	4.815365
292.715484	7999.862189	11.032704	-0.059564	4.815358
292.898410	7999.778648	11.037709	-0.059598	4.815333
292.834150	7999.853470	11.042714	-0.059586	4.815355
292.799781	7999.958711	11.047719	-0.059580	4.815386
292.833568	7999.767965	11.052723	-0.059586	4.815330
292.674536	7999.966263	11.057728	-0.059557	4.815389
292.981155	7999.774685	11.062733	-0.059614	4.815331
292.931746	7999.992967	11.067738	-0.059605	4.815395
292.758683	7999.851168	11.072743	-0.059572	4.815355
292.833637	7999.972112	11.077747	-0.059586	4.815390
292.693440	7999.961245	11.082752	-0.059560	4.815387
292.940484	7999.979228	11.087757	-0.059606	4.815391
293.026025	7999.874838	11.092762	-0.059622	4.815360
292.940576	7999.985647	11.097767	-0.059606	4.815393
292.930341	7999.857228	11.102771	-0.059604	4.815356
292.937913	7999.850944	11.107776	-0.059606	4.815354
293.126662	7999.952395	11.112781	-0.059641	4.815383
292.947832	7999.863938	11.117786	-0.059608	4.815358
292.825247	8000.008334	11.122791	-0.059585	4.815400
293.021331	7999.780727	11.127795	-0.059621	4.815333
292.927140	8000.061326	11.132800	-0.059604	4.815415
292.858920	7999.763083	11.137805	-0.059591	4.815329
292.916199	7999.874115	11.142810	-0.059602	4.815361
292.848915	7999.869798	11.147815	-0.059590	4.815360
293.147552	7999.780689	11.152819	-0.059645	4.815332
292.960220	7999.860957	11.157824	-0.059610	4.815357
292.900706	7999.979677	11.162829	-0.059599	4.815392
292.888356	7999.849085	11.167834	-0.059597	4.815354
292.777852	7999.857948	11.172839	-0.059576	4.815357
292.949195	7999.812690	11.177843	-0.059608	4.815343
293.034025	7999.918835	11.182848	-0.059624	4.815373
293.060451	7999.877593	11.187853	-0.059629	4.815361
292.895625	7999.934719	11.192858	-0.059599	4.815379
293.034754	7999.856866	11.197863	-0.059624	4.815355
293.061277	7999.765394	11.202867	-0.059629	4.815328
292.828890	7999.978511	11.207872	-0.059586	4.815392
293.204916	7999.762431	11.212877	-0.059656	4.815327
292.928656	7999.875428	11.217882	-0.059605	4.815361
292.781409	7999.865513	11.222887	-0.059577	4.815359
292.936035	7999.888380	11.227891	-0.059606	4.815365
292.936107	7999.846702	11.232896	-0.059606	4.815353
292.942930	7999.897049	11.237901	-0.059608	4.815367
292.928137	7999.858331	11.242906	-0.059605	4.815356
293.025998	7999.886672	11.247911	-0.059623	4.815364
293.200137	7999.851079	11.252915	-0.059656	4.815353
293.061441	7999.972765	11.257920	-0.059630	4.815389
293.082171	7999.897228	11.262925	-0.059634	4.815367
292.990520	7999.856170	11.267930	-0.059617	4.815355
293.030060	7999.967978	11.272935	-0.059624	4.815388
293.126442	7999.857354	11.277939	-0.059642	4.815355
292.918560	7999.843231	11.282944	-0.059603	4.815352
293.091258	7999.987167	11.287949	-0.059636	4.815393
292.855986	7999.842201	11.292954	-0.059592	4.815352
292.817945	7999.985857	11.297959	-0.059585	4.815394
293.015182	7999.967747	11.302963	-0.059621	4.815388
292.817390	7999.982646	11.307968	-0.059585	4.815393
292.942001	7999.868215	11.312973	-0.059608	4.815359
293.055999	7999.844453	11.317978	-0.059629	4.815351
292.997372	8000.136329	11.322983	-0.059618	4.815437
292.861901	7999.763228	11.327987	-0.059593	4.815329
292.918428	7999.954405	11.332992	-0.059604	4.815384
292.952402	7999.897256	11.337997	-0.059610	4.815367
292.770062	7999.853630	11.343002	-0.059576	4.815355
292.896328	7999.865340	11.348007	-0.059599	4.815358
293.116936	7999.876473	11.353011	-0.059641	4.815360
293.050450	7999.966221	11.358016	-0.059628	4.815387
293.175813	7999.861420	11.363021	-0.059652	4.815356
293.255434	7999.876634	11.368026	-0.059666	4.815360
293.189056	7999.860576	11.373031	-0.059654	4.815355
293.373523	7999.793091	11.378035	-0.059688	4.815335
293.080378	7999.850233	11.383040	-0.059634	4.815353
293.187517	7999.862695	11.388045	-0.059654	4.815356
293.130876	7999.774122	11.393050	-0.059643	4.815331
292.960370	7999.874974	11.398055	-0.059612	4.815361
293.041719	7999.972512	11.403059	-0.059627	4.815389
293.024460	7999.882452	11.408064	-0.059624	4.815363
293.020187	7999.884521	11.413069	-0.059623	4.815363
292.847319	7999.754482	11.418074	-0.059591	4.815326
293.020534	7999.885601	11.423079	-0.059623	4.815364
292.940043	7999.867172	11.428083	-0.059608	4.815359
293.180373	7999.879700	11.433088	-0.059653	4.815361
293.160502	7999.839829	11.438093	-0.059649	4.815350
293.040301	7999.812193	11.443098	-0.059627	4.815342
293.051642	8000.098814	11.448103	-0.059629	4.815426
293.169528	7999.959689	11.453107	-0.059651	4.815385
292.935378	8000.017806	11.458112	-0.059607	4.815403
293.015654	7999.995624	11.463117	-0.059622	4.815396
293.040089	7999.872053	11.468122	-0.059627	4.815360
293.139256	8000.088520	11.473127	-0.059646	4.815422
293.124987	7999.772999	11.478131	-0.059643	4.815330
293.020032	7999.940130	11.483136	-0.059623	4.815380
293.225169	7999.902913	11.488141	-0.059662	4.815368
293.056328	7999.752633	11.493146	-0.059630	4.815325
293.075539	7999.871586	11.498151	-0.059634	4.815359
293.027502	7999.862244	11.503155	-0.059625	4.815357
293.064897	7999.868209	11.508160	-0.059632	4.815358
293.006599	7999.886485	11.513165	-0.059621	4.815364
293.083443	7999.871727	11.518170	-0.059635	4.815359
292.940398	7999.985859	11.523175	-0.059609	4.815393
293.214095	7999.858930	11.528179	-0.059660	4.815355
293.130488	7999.990078	11.533184	-0.059644	4.815394
293.245013	7999.875479	11.538189	-0.059666	4.815360
293.050862	7999.860513	11.543194	-0.059629	4.815356
292.950993	7999.966809	11.548199	-0.059611	4.815388
293.039005	7999.987505	11.553203	-0.059627	4.815393
293.057863	7999.847811	11.558208	-0.059631	4.815352
293.007140	7999.962401	11.563213	-0.059621	4.815386
293.026665	7999.789587	11.568218	-0.059625	4.815335
293.148331	7999.842903	11.573223	-0.059648	4.815350
293.142157	7999.796846	11.578227	-0.059647	4.815337
293.016623	7999.863173	11.583232	-0.059623	4.815357
293.140116	7999.866287	11.588237	-0.059646	4.815357
293.079205	7999.837494	11.593242	-0.059635	4.815349
293.005163	8000.012619	11.598247	-0.059621	4.815401
293.203593	7999.833144	11.603251	-0.059658	4.815347
293.144693	7999.866373	11.608256	-0.059647	4.815357
292.976132	7999.778086	11.613261	-0.059616	4.815332
293.016738	7999.877086	11.618266	-0.059623	4.815361
293.224053	7999.853799	11.623271	-0.059662	4.815353
293.123181	7999.887402	11.628275	-0.059643	4.815364
293.257175	7999.854352	11.633280	-0.059668	4.815353
293.135709	7999.978460	11.638285	-0.059646	4.815390
293.157150	7999.782164	11.643290	-0.059650	4.815333
293.009442	7999.866293	11.648295	-0.059622	4.815358
293.208355	7999.765916	11.653299	-0.059659	4.815328
293.199948	7999.946401	11.658304	-0.059658	4.815380
293.105845	7999.782394	11.663309	-0.059640	4.815333
293.287993	8000.040847	11.668314	-0.059674	4.815408
293.225904	7999.967145	11.673319	-0.059663	4.815386
293.084902	7999.931683	11.678323	-0.059637	4.815377
293.173003	8000.001545	11.683328	-0.059653	4.815397
293.278862	7999.923140	11.688333	-0.059673	4.815373
293.181343	7999.889466	11.693338	-0.059655	4.815364
293.174510	7999.866912	11.698343	-0.059653	4.815357
293.367903	7999.779268	11.703347	-0.059689	4.815331
293.271609	7999.972194	11.708352	-0.059671	4.815388
293.252789	8000.006086	11.713357	-0.059668	4.815398
293.376409	7999.853161	11.718362	-0.059691	4.815352
293.322415	7999.787076	11.723367	-0.059681	4.815333
293.404752	7999.841879	11.728371	-0.059696	4.815349
293.155738	7999.955327	11.733376	-0.059650	4.815383
293.090093	7999.871948	11.738381	-0.059638	4.815359
293.342463	7999.857956	11.743386	-0.059685	4.815354
293.240663	7999.872306	11.748391	-0.059666	4.815359
293.235892	7999.777109	11.753395	-0.059665	4.815331
293.332818	7999.758409	11.758400	-0.059683	4.815325
293.343735	7999.874019	11.763405	-0.059685	4.815359
293.375782	7999.866002	11.768410	-0.059691	4.815356
293.303222	7999.864804	11.773415	-0.059678	4.815356
293.442253	7999.889551	11.778419	-0.059704	4.815363
293.317071	7999.855419	11.783424	-0.059680	4.815353
293.173917	7999.865878	11.788429	-0.059654	4.815357
293.243942	7999.980330	11.793434	-0.059667	4.815390
293.210995	7999.859015	11.798439	-0.059661	4.815355
293.421895	7999.784487	11.803443	-0.059700	4.815332
293.339878	7999.865428	11.808448	-0.059685	4.815356
293.265214	7999.776556	11.813453	-0.059671	4.815331
293.493352	7999.896829	11.818458	-0.059713	4.815365
293.400088	7999.777723	11.823463	-0.059696	4.815330
293.495262	7999.877628	11.828467	-0.059714	4.815359
293.207731	7999.775615	11.833472	-0.059660	4.815331
293.271540	7999.794842	11.838477	-0.059672	4.815336
293.311053	7999.869244	11.843482	-0.059680	4.815357
293.122190	7999.877878	11.848487	-0.059644	4.815361
293.209116	7999.879319	11.853491	-0.059661	4.815361
293.353966	7999.962945	11.858496	-0.059688	4.815385
293.262862	7999.870594	11.863501	-0.059671	4.815358
293.197876	7999.868453	11.868506	-0.059659	4.815358
293.452563	7999.881219	11.873511	-0.059706	4.815360
293.353940	7999.773781	11.878515	-0.059688	4.815329
293.155822	7999.866696	11.883520	-0.059651	4.815357
293.025778	7999.904091	11.888525	-0.059627	4.815369
293.152575	7999.846340	11.893530	-0.059650	4.815351
293.177489	7999.862787	11.898535	-0.059655	4.815356
293.361171	7999.870103	11.903539	-0.059689	4.815357
293.374896	7999.984692	11.908544	-0.059692	4.815391
293.509406	7999.968751	11.913549	-0.059717	4.815385
293.365324	7999.862698	11.918554	-0.059690	4.815355
293.195873	7999.968912	11.923559	-0.059659	4.815387
293.417252	7999.774854	11.928563	-0.059700	4.815329
293.296112	7999.963094	11.933568	-0.059677	4.815385
293.217369	7999.894461	11.938573	-0.059663	4.815365
293.465959	7999.867582	11.943578	-0.059709	4.815356
293.314111	7999.779570	11.948583	-0.059681	4.815331
293.268092	7999.867520	11.953587	-0.059672	4.815357
293.146267	7999.854819	11.958592	-0.059649	4.815354
293.358555	7999.870090	11.963597	-0.059689	4.815357
293.197611	7999.896287	11.968602	-0.059659	4.815366
293.149653	7999.879464	11.973607	-0.059650	4.815361
293.261697	7999.822538	11.978611	-0.059671	4.815344
293.214892	7999.917956	11.983616	-0.059662	4.815372
293.232707	7999.889396	11.988621	-0.059666	4.815364
293.408821	7999.858112	11.993626	-0.059699	4.815354
293.453133	7999.976413	11.998631	-0.059707	4.815388
293.426357	7999.963147	12.003635	-0.059702	4.815384
293.304722	8000.023126	12.008640	-0.059679	4.815402
293.378430	7999.976253	12.013645	-0.059693	4.815388
293.441471	7999.990124	12.018650	-0.059705	4.815392
293.408475	7999.920110	12.023655	-0.059699	4.815372
293.561121	7999.805073	12.028659	-0.059727	4.815337
293.441747	7999.877914	12.033664	-0.059705	4.815359
293.353899	7999.985479	12.038669	-0.059689	4.815391
293.446094	7999.866235	12.043674	-0.059706	4.815356
293.562259	7999.949387	12.048679	-0.059728	4.815380
293.401513	7999.866571	12.053683	-0.059698	4.815356
293.382379	7999.870532	12.058688	-0.059694	4.815357
293.404647	7999.879453	12.063693	-0.059698	4.815360
293.591431	7999.876134	12.068698	-0.059733	4.815358
293.534843	7999.847412	12.073703	-0.059722	4.815350
293.537374	7999.881657	12.078707	-0.059723	4.815360
293.584121	7999.977555	12.083712	-0.059732	4.815388
293.544285	8000.020718	12.088717	-0.059724	4.815400
293.383179	7999.853463	12.093722	-0.059694	4.815352
293.343297	7999.916932	12.098727	-0.059687	4.815371
293.338908	7999.809984	12.103731	-0.059686	4.815340
293.291938	7999.967388	12.108736	-0.059678	4.815386
293.372303	7999.889631	12.113741	-0.059692	4.815363
293.654650	7999.956295	12.118746	-0.059745	4.815381
293.605955	7999.992899	12.123751	-0.059736	4.815392
293.831723	7999.861971	12.128755	-0.059778	4.815353
293.586474	7999.985100	12.133760	-0.059733	4.815390
293.332384	7999.961660	12.138765	-0.059685	4.815384
293.508042	7999.873723	12.143770	-0.059718	4.815358
293.559093	7999.862814	12.148775	-0.059727	4.815354
293.586380	7999.867543	12.153779	-0.059733	4.815355
293.535874	7999.980000	12.158784	-0.059723	4.815389
293.491987	7999.952557	12.163789	-0.059715	4.815381
293.456462	8000.021443	12.168794	-0.059709	4.815401
293.179390	8000.022204	12.173799	-0.059657	4.815403
293.446389	8000.012731	12.178803	-0.059707	4.815399
293.664594	7999.976799	12.183808	-0.059747	4.815387
293.648219	7999.993631	12.188813	-0.059744	4.815392
293.775476	7999.774501	12.193818	-0.059768	4.815327
293.719663	7999.868702	12.198823	-0.059758	4.815355
293.700821	7999.781822	12.203827	-0.059754	4.815330
293.482411	7999.871194	12.208832	-0.059714	4.815357
293.545270	7999.877581	12.213837	-0.059725	4.815359
293.558025	7999.864969	12.218842	-0.059728	4.815355
293.444972	7999.980667	12.223847	-0.059707	4.815389
293.374282	7999.879034	12.228851	-0.059693	4.815360
293.602723	7999.920224	12.233856	-0.059736	4.815371
293.532842	7999.864562	12.238861	-0.059723	4.815355
293.548512	7999.857343	12.243866	-0.059726	4.815353
293.603853	7999.998271	12.248871	-0.059736	4.815394
293.649410	7999.962689	12.253875	-0.059745	4.815383
293.511724	7999.967895	12.258880	-0.059719	4.815385
293.387986	7999.865384	12.263885	-0.059696	4.815356
293.612898	7999.994156	12.268890	-0.059738	4.815392
293.389425	8000.010767	12.273895	-0.059697	4.815398
293.349528	7999.861549	12.278899	-0.059689	4.815355
293.627433	8000.111971	12.283904	-0.059741	4.815427
293.560736	7999.954827	12.288909	-0.059729	4.815381
293.214079	8000.038871	12.293914	-0.059664	4.815407
293.418572	8000.005918	12.298919	-0.059702	4.815397
293.537866	7999.966212	12.303923	-0.059724	4.815385
293.620562	8000.008197	12.308928	-0.059740	4.815396
293.667515	7999.880723	12.313933	-0.059749	4.815359
293.783385	7999.861267	12.318938	-0.059770	4.815353
293.540942	8000.095597	12.323943	-0.059725	4.815422
293.674550	7999.888328	12.328947	-0.059750	4.815361
293.767655	7999.995681	12.333952	-0.059767	4.815392
293.646024	7999.979777	12.338957	-0.059745	4.815388
293.672001	7999.879743	12.343962	-0.059750	4.815359
293.594414	8000.064431	12.348967	-0.059735	4.815413
293.521914	7999.903984	12.353971	-0.059722	4.815366
293.477129	7999.983404	12.358976	-0.059713	4.815390
293.601674	7999.940579	12.363981	-0.059737	4.815377
293.772145	7999.852556	12.368986	-0.059768	4.815350
293.559465	7999.891790	12.373991	-0.059729	4.815363
293.659642	7999.774816	12.378995	-0.059747	4.815328
293.477130	7999.982348	12.384000	-0.059714	4.815390
293.472011	7999.866838	12.389005	-0.059713	4.815356
293.358546	7999.868169	12.394010	-0.059691	4.815357
293.335416	7999.996043	12.399015	-0.059687	4.815394
293.679306	7999.956847	12.404019	-0.059751	4.815381
293.510723	7999.942303	12.409024	-0.059720	4.815378
293.678009	8000.030577	12.414029	-0.059751	4.815403
293.606463	8000.009088	12.419034	-0.059738	4.815397
293.442891	7999.985008	12.424039	-0.059707	4.815390
293.630390	7999.897267	12.429043	-0.059742	4.815364
293.715984	7999.987395	12.434048	-0.059758	4.815390
293.826595	7999.883418	12.439053	-0.059779	4.815359
293.813434	7999.872515	12.444058	-0.059776	4.815356
293.849740	7999.965034	12.449063	-0.059783	4.815383
294.061474	7999.861662	12.454067	-0.059823	4.815351
293.820270	7999.899355	12.459072	-0.059778	4.815364
293.708123	7999.935978	12.464077	-0.059757	4.815375
293.652500	7999.766193	12.469082	-0.059747	4.815326
293.690356	8000.074632	12.474087	-0.059754	4.815415
293.653239	7999.879501	12.479091	-0.059747	4.815359
293.540534	7999.978104	12.484096	-0.059726	4.815388
293.513118	7999.982997	12.489101	-0.059721	4.815390
293.634343	7999.870645	12.494106	-0.059743	4.815356
293.471886	7999.976976	12.499111	-0.059713	4.815388
293.645504	7999.775714	12.504115	-0.059745	4.815328
293.493025	7999.875796	12.509120	-0.059717	4.815358
293.431445	7999.985933	12.514125	-0.059706	4.815391
293.723967	7999.765263	12.519130	-0.059760	4.815325
293.646556	8000.004461	12.524135	-0.059746	4.815395
293.563678	7999.844912	12.529139	-0.059730	4.815349
293.729213	7999.894680	12.534144	-0.059761	4.815363
293.848450	7999.773745	12.539149	-0.059783	4.815327
293.607100	7999.868082	12.544154	-0.059739	4.815355
293.677926	7999.873532	12.549159	-0.059752	4.815357
293.837544	7999.765022	12.554163	-0.059782	4.815324
293.840805	7999.867682	12.559168	-0.059782	4.815354
293.746175	7999.884288	12.564173	-0.059765	4.815360
293.828846	7999.971162	12.569178	-0.059780	4.815385
293.654616	7999.915910	12.574183	-0.059748	4.815369
293.655470	7999.815461	12.579187	-0.059748	4.815340
293.718134	7999.967199	12.584192	-0.059760	4.815384
293.780135	7999.859212	12.589197	-0.059771	4.815352
293.763093	7999.856795	12.594202	-0.059768	4.815351
293.535848	8000.000529	12.599207	-0.059726	4.815395
293.712902	7999.865588	12.604211	-0.059759	4.815354
293.651725	7999.778007	12.609216	-0.059747	4.815329
293.732574	7999.876607	12.614221	-0.059762	4.815357
293.761657	7999.862127	12.619226	-0.059768	4.815353
293.686424	7999.860885	12.624231	-0.059754	4.815353
293.725709	7999.873294	12.629235	-0.059761	4.815356
293.764508	7999.875007	12.634240	-0.059768	4.815357
293.526398	7999.979017	12.639245	-0.059724	4.815388
293.674808	7999.854290	12.644250	-0.059752	4.815351
293.433271	7999.979619	12.649255	-0.059707	4.815389
293.610964	7999.766668	12.654259	-0.059740	4.815326
293.536342	7999.965298	12.659264	-0.059726	4.815384
293.456603	7999.949018	12.664269	-0.059711	4.815380
293.689307	7999.805379	12.669274	-0.059755	4.815337
293.658931	7999.855111	12.674279	-0.059749	4.815351
293.855157	7999.878668	12.679283	-0.059786	4.815357
293.674284	7999.962249	12.684288	-0.059752	4.815383
293.899548	7999.968117	12.689293	-0.059794	4.815383
293.907486	7999.864578	12.694298	-0.059795	4.815353
293.904987	7999.988519	12.699303	-0.059795	4.815389
293.901264	7999.818523	12.704307	-0.059794	4.815340
293.624997	7999.903732	12.709312	-0.059743	4.815366
293.674267	7999.960126	12.714317	-0.059752	4.815382
293.829132	7999.817337	12.719322	-0.059781	4.815340
293.646598	7999.926541	12.724327	-0.059747	4.815372
293.626326	7999.769097	12.729331	-0.059743	4.815326
293.738857	7999.872496	12.734336	-0.059764	4.815356
293.629479	7999.888858	12.739341	-0.059744	4.815361
293.602523	7999.859557	12.744346	-0.059739	4.815353
293.451429	7999.960732	12.749351	-0.059711	4.815383
293.817508	7999.884495	12.754355	-0.059779	4.815359
293.921252	7999.871252	12.759360	-0.059798	4.815355
293.736011	7999.885289	12.764365	-0.059764	4.815360
293.641513	7999.864490	12.769370	-0.059746	4.815354
293.960931	7999.870847	12.774375	-0.059806	4.815355
293.785616	7999.960933	12.779379	-0.059773	4.815382
293.795684	7999.930107	12.784384	-0.059775	4.815373
293.853700	8000.025124	12.789389	-0.059786	4.815400
293.926011	7999.868142	12.794394	-0.059799	4.815354
293.789598	7999.958871	12.799399	-0.059774	4.815381
293.653353	7999.866841	12.804403	-0.059749	4.815355
293.849115	7999.850845	12.809408	-0.059785	4.815349
293.665514	7999.965376	12.814413	-0.059751	4.815384
293.700540	7999.862286	12.819418	-0.059758	4.815353
293.762564	7999.987294	12.824423	-0.059769	4.815390
293.832057	7999.819578	12.829427	-0.059782	4.815340
293.751013	8000.079024	12.834432	-0.059767	4.815416
293.739285	7999.995467	12.839437	-0.059765	4.815392
293.799340	7999.971881	12.844442	-0.059776	4.815385
293.606361	8000.018923	12.849447	-0.059740	4.815399
293.752805	7999.774459	12.854451	-0.059767	4.815327
293.877660	7999.957153	12.859456	-0.059791	4.815380
293.768791	7999.962835	12.864461	-0.059771	4.815382
293.617951	7999.894077	12.869466	-0.059743	4.815363
293.501065	7999.974441	12.874471	-0.059721	4.815387
293.709544	7999.933005	12.879475	-0.059760	4.815374
293.707603	8000.054818	12.884480	-0.059759	4.815409
293.652194	7999.913891	12.889485	-0.059749	4.815369
293.725292	8000.138482	12.894490	-0.059763	4.815434
293.613462	8000.031891	12.899495	-0.059742	4.815403
293.749267	7999.967876	12.904499	-0.059767	4.815384
293.710680	7999.998235	12.909504	-0.059760	4.815393
293.671659	7999.980491	12.914509	-0.059753	4.815388
293.654318	7999.966312	12.919514	-0.059750	4.815384
293.751864	7999.957241	12.924519	-0.059768	4.815381
293.854781	7999.903370	12.929523	-0.059787	4.815365
293.649822	7999.929907	12.934528	-0.059749	4.815373
293.690608	7999.970129	12.939533	-0.059756	4.815385
293.827071	7999.852686	12.944538	-0.059782	4.815350
293.778271	7999.866844	12.949543	-0.059773	4.815354
294.071396	7999.885592	12.954547	-0.059827	4.815358
294.014658	7999.877174	12.959552	-0.059817	4.815356
293.996374	7999.892905	12.964557	-0.059814	4.815361
293.816687	7999.809775	12.969562	-0.059780	4.815337
293.795274	7999.918440	12.974567	-0.059776	4.815369
293.829585	7999.854883	12.979571	-0.059783	4.815350
293.768065	7999.970365	12.984576	-0.059771	4.815385
293.728543	7999.961163	12.989581	-0.059764	4.815382
293.777681	7999.875407	12.994586	-0.059773	4.815357
293.817034	7999.973321	12.999591	-0.059780	4.815385
293.904382	7999.876440	13.004595	-0.059797	4.815356
293.984250	7999.858526	13.009600	-0.059811	4.815351
293.865265	8000.037186	13.014605	-0.059789	4.815404
293.879614	7999.935890	13.019610	-0.059792	4.815374
293.792331	7999.956893	13.024615	-0.059776	4.815380
293.766539	7999.864553	13.029619	-0.059771	4.815354
293.712702	7999.858320	13.034624	-0.059761	4.815352
293.663041	7999.886358	13.039629	-0.059752	4.815360
293.960481	7999.869907	13.044634	-0.059807	4.815354
293.778029	8000.000489	13.049639	-0.059773	4.815393
293.866589	7999.871565	13.054643	-0.059790	4.815355
294.094802	7999.858243	13.059648	-0.059832	4.815350
293.944815	7999.882483	13.064653	-0.059804	4.815358
293.819412	7999.866516	13.069658	-0.059781	4.815354
294.118390	7999.874673	13.074663	-0.059837	4.815355
294.190956	7999.861982	13.079667	-0.059850	4.815351
294.085544	7999.860240	13.084672	-0.059831	4.815351
293.968434	7999.772802	13.089677	-0.059809	4.815326
294.173133	7999.778329	13.094682	-0.059847	4.815326
293.899348	7999.858235	13.099687	-0.059796	4.815351
293.976779	7999.870207	13.104691	-0.059811	4.815354
293.972012	7999.998386	13.109696	-0.059810	4.815392
293.934451	7999.952877	13.114701	-0.059803	4.815379
293.848481	7999.883055	13.119706	-0.059787	4.815359
294.014177	7999.856942	13.124711	-0.059818	4.815350
294.072615	7999.853636	13.129715	-0.059829	4.815349
293.933605	7999.885540	13.134720	-0.059803	4.815359
293.849229	7999.861701	13.139725	-0.059787	4.815352
293.933801	7999.876998	13.144730	-0.059803	4.815356
293.918204	7999.970796	13.149735	-0.059800	4.815384
293.910720	7999.872346	13.154739	-0.059799	4.815355
293.890306	7999.852772	13.159744	-0.059795	4.815350
293.792167	8000.018951	13.164749	-0.059777	4.815399
293.793851	7999.838356	13.169754	-0.059777	4.815346
293.921281	7999.989029	13.174759	-0.059801	4.815389
294.159553	7999.781354	13.179763	-0.059845	4.815327
293.941125	7999.995775	13.184768	-0.059805	4.815391
293.683922	7999.903880	13.189773	-0.059757	4.815365
293.830820	7999.896694	13.194778	-0.059784	4.815363
293.825911	7999.893409	13.199783	-0.059783	4.815362
294.059801	7999.882319	13.204787	-0.059827	4.815357
293.794061	7999.878993	13.209792	-0.059777	4.815358
293.930925	7999.864160	13.214797	-0.059803	4.815353
293.959698	7999.878533	13.219802	-0.059808	4.815357
293.940638	7999.763860	13.224807	-0.059805	4.815323
293.986615	7999.982656	13.229811	-0.059813	4.815387
294.127136	7999.888793	13.234816	-0.059839	4.815359
293.914576	7999.953680	13.239821	-0.059800	4.815379
294.126112	7999.847098	13.244826	-0.059839	4.815347
294.046763	7999.906709	13.249831	-0.059825	4.815365
293.913156	7999.861748	13.254835	-0.059800	4.815352
293.850547	7999.869265	13.259840	-0.059788	4.815355
293.818450	8000.036537	13.264845	-0.059782	4.815404
294.003007	7999.868587	13.269850	-0.059816	4.815354
293.839536	7999.860540	13.274855	-0.059786	4.815352
293.946472	7999.975604	13.279859	-0.059806	4.815385
294.035407	7999.762252	13.284864	-0.059823	4.815322
293.893534	7999.878542	13.289869	-0.059796	4.815357
293.898797	8000.007956	13.294874	-0.059797	4.815395
293.895460	7999.855066	13.299879	-0.059797	4.815350
294.078284	7999.979936	13.304883	-0.059831	4.815386
293.896625	7999.861503	13.309888	-0.059797	4.815352
293.994887	7999.850306	13.314893	-0.059815	4.815348
293.942008	7999.869740	13.319898	-0.059805	4.815354
293.754252	7999.846329	13.324903	-0.059770	4.815348
293.839187	7999.772922	13.329907	-0.059786	4.815326
293.985598	7999.882226	13.334912	-0.059814	4.815358
293.964522	7999.767519	13.339917	-0.059810	4.815324
294.125315	7999.884543	13.344922	-0.059840	4.815358
293.999687	7999.865366	13.349927	-0.059816	4.815353
293.867638	7999.869596	13.354931	-0.059792	4.815355
293.963975	7999.756833	13.359936	-0.059810	4.815321
294.137182	7999.964910	13.364941	-0.059842	4.815381
294.093517	7999.866929	13.369946	-0.059834	4.815353
293.813796	7999.980938	13.374951	-0.059782	4.815387
293.958699	7999.922418	13.379955	-0.059809	4.815370
293.986105	7999.975245	13.384960	-0.059814	4.815385
293.840984	7999.956813	13.389965	-0.059787	4.815380
294.061633	7999.986119	13.394970	-0.059828	4.815388
293.970050	7999.963230	13.399975	-0.059811	4.815381
293.834811	7999.868009	13.404979	-0.059786	4.815354
294.019096	8000.084821	13.409984	-0.059820	4.815417
293.967990	7999.979235	13.414989	-0.059811	4.815386
294.155025	7999.941719	13.419994	-0.059846	4.815374
293.957439	8000.062432	13.424999	-0.059809	4.815410
293.996593	7999.992542	13.430003	-0.059816	4.815390
293.921061	7999.994500	13.435008	-0.059802	4.815391
294.101266	7999.999623	13.440013	-0.059836	4.815391
294.174621	7999.776393	13.445018	-0.059849	4.815326
294.115066	7999.981687	13.450023	-0.059838	4.815386
294.039616	7999.990060	13.455027	-0.059824	4.815389
294.064676	7999.882529	13.460032	-0.059829	4.815357
294.165639	7999.773048	13.465037	-0.059848	4.815325
294.348708	7999.880822	13.470042	-0.059882	4.815355
294.066487	7999.983033	13.475047	-0.059830	4.815387
294.184564	7999.864216	13.480051	-0.059851	4.815351
294.213614	7999.994024	13.485056	-0.059857	4.815389
294.105631	7999.858640	13.490061	-0.059837	4.815350
294.103001	7999.892800	13.495066	-0.059836	4.815360
294.034090	7999.979303	13.500071	-0.059824	4.815386
294.110507	7999.861934	13.505075	-0.059838	4.815351
293.983397	7999.959231	13.510080	-0.059814	4.815380
293.966299	7999.853140	13.515085	-0.059811	4.815349
293.996954	7999.861131	13.520090	-0.059817	4.815351
293.910442	7999.968719	13.525095	-0.059801	4.815383
294.161472	7999.978221	13.530099	-0.059848	4.815385
294.229446	7999.870331	13.535104	-0.059860	4.815353
294.164318	7999.976135	13.540109	-0.059848	4.815384
294.021138	7999.881851	13.545114	-0.059821	4.815357
294.052654	8000.003149	13.550119	-0.059827	4.815393
293.994449	7999.994707	13.555123	-0.059817	4.815390
294.152290	7999.877617	13.560128	-0.059846	4.815355
294.072177	7999.990655	13.565133	-0.059831	4.815389
294.224475	7999.862784	13.570138	-0.059859	4.815351
293.992500	7999.973309	13.575143	-0.059816	4.815384
294.181918	7999.771238	13.580147	-0.059851	4.815324
294.184786	7999.888855	13.585152	-0.059852	4.815359
294.148500	7999.852987	13.590157	-0.059845	4.815348
294.223334	7999.865985	13.595162	-0.059859	4.815352
294.002459	7999.963867	13.600167	-0.059818	4.815381
294.166703	7999.873603	13.605171	-0.059849	4.815354
294.240803	7999.871625	13.610176	-0.059863	4.815353
293.910919	7999.976254	13.615181	-0.059801	4.815385
294.191113	7999.864395	13.620186	-0.059853	4.815351
294.141520	7999.873196	13.625191	-0.059844	4.815354
294.227166	7999.873547	13.630195	-0.059860	4.815354
294.316472	7999.868615	13.635200	-0.059877	4.815352
294.167398	7999.886457	13.640205	-0.059849	4.815358
293.983257	7999.765846	13.645210	-0.059815	4.815324
294.092694	7999.982487	13.650215	-0.059835	4.815386
294.051981	7999.879211	13.655219	-0.059828	4.815356
294.101157	7999.872546	13.660224	-0.059837	4.815354
294.132688	7999.869864	13.665229	-0.059843	4.815353
294.120137	7999.886759	13.670234	-0.059841	4.815358
294.101733	7999.884319	13.675239	-0.059837	4.815358
294.198617	7999.937228	13.680243	-0.059855	4.815373
294.298379	7999.908955	13.685248	-0.059874	4.815364
294.116440	8000.005345	13.690253	-0.059840	4.815393
294.129898	7999.866626	13.695258	-0.059843	4.815352
294.070021	7999.872051	13.700263	-0.059831	4.815354
294.274754	7999.972702	13.705267	-0.059870	4.815383
294.059121	7999.860118	13.710272	-0.059829	4.815351
293.832171	7999.889498	13.715277	-0.059787	4.815360
294.175253	7999.781886	13.720282	-0.059851	4.815327
293.979841	7999.857745	13.725287	-0.059815	4.815350
293.951699	7999.875451	13.730291	-0.059810	4.815356
294.080270	7999.962017	13.735296	-0.059834	4.815380
293.962438	7999.923730	13.740301	-0.059812	4.815370
294.035296	7999.842641	13.745306	-0.059825	4.815346
294.022595	8000.029473	13.750311	-0.059823	4.815400
294.135250	8000.015308	13.755315	-0.059844	4.815396
294.253630	7999.884739	13.760320	-0.059866	4.815357
294.119609	7999.965889	13.765325	-0.059841	4.815381
294.369834	7999.928351	13.770330	-0.059888	4.815369
294.152641	7999.917276	13.775335	-0.059847	4.815367
293.931238	7999.986293	13.780339	-0.059806	4.815388
294.126094	7999.780037	13.785344	-0.059842	4.815327
294.167475	7999.972038	13.790349	-0.059850	4.815383
294.089020	7999.873482	13.795354	-0.059835	4.815355
294.133776	7999.999274	13.800359	-0.059844	4.815391
294.200572	7999.973663	13.805363	-0.059856	4.815383
294.405405	7999.858419	13.810368	-0.059894	4.815349
294.029108	7999.967623	13.815373	-0.059824	4.815382
294.119121	7999.857961	13.820378	-0.059841	4.815350
294.097686	8000.010446	13.825383	-0.059837	4.815395
294.050128	7999.886750	13.830387	-0.059828	4.815359
293.961849	7999.817958	13.835392	-0.059812	4.815339
293.903199	7999.921731	13.840397	-0.059801	4.815370
294.033814	7999.873662	13.845402	-0.059825	4.815355
293.887326	7999.856277	13.850407	-0.059798	4.815350
294.092141	7999.963343	13.855411	-0.059836	4.815381
294.040714	7999.874853	13.860416	-0.059827	4.815355
293.930097	7999.863405	13.865421	-0.059806	4.815352
294.060876	7999.888017	13.870426	-0.059831	4.815359
294.342362	7999.856339	13.875431	-0.059883	4.815348
294.297125	7999.982780	13.880435	-0.059875	4.815385
294.326365	7999.893487	13.885440	-0.059880	4.815359
294.321943	7999.960751	13.890445	-0.059879	4.815379
294.325892	7999.889209	13.895450	-0.059880	4.815358
293.919135	7999.958364	13.900455	-0.059804	4.815380
294.238407	7999.909142	13.905459	-0.059864	4.815364
294.278523	7999.863851	13.910464	-0.059871	4.815351
294.236815	7999.880264	13.915469	-0.059864	4.815356
294.235308	7999.780843	13.920474	-0.059863	4.815327
294.126764	7999.888066	13.925479	-0.059843	4.815359
294.007341	7999.862579	13.930483	-0.059821	4.815352
294.138599	7999.787801	13.935488	-0.059845	4.815329
294.123867	7999.971392	13.940493	-0.059843	4.815383
294.327776	7999.783455	13.945498	-0.059881	4.815327
294.318709	7999.875224	13.950503	-0.059879	4.815354
294.258450	7999.780175	13.955507	-0.059868	4.815326
294.285123	7999.870398	13.960512	-0.059873	4.815353
294.229684	7999.992395	13.965517	-0.059863	4.815389
294.343001	7999.774100	13.970522	-0.059884	4.815324
294.219630	7999.873597	13.975527	-0.059861	4.815354
294.310987	7999.971303	13.980531	-0.059878	4.815382
294.317473	7999.870946	13.985536	-0.059879	4.815353
294.101208	7999.938978	13.990541	-0.059839	4.815374
294.329717	7999.938488	13.995546	-0.059881	4.815372
294.189362	7999.882727	14.000551	-0.059855	4.815357
294.153043	7999.863959	14.005555	-0.059849	4.815351
294.390829	7999.884998	14.010560	-0.059893	4.815356
294.148681	7999.870305	14.015565	-0.059848	4.815353
294.098216	7999.881229	14.020570	-0.059838	4.815357
294.128718	7999.858223	14.025575	-0.059844	4.815350
294.329854	7999.990880	14.030579	-0.059882	4.815388
294.138779	7999.860532	14.035584	-0.059846	4.815350
294.148125	7999.886340	14.040589	-0.059848	4.815358
294.390398	7999.778129	14.045594	-0.059893	4.815325
294.193095	7999.869989	14.050599	-0.059856	4.815353
294.183924	7999.879459	14.055603	-0.059855	4.815356
294.466098	7999.778321	14.060608	-0.059907	4.815325
294.396049	7999.890456	14.065613	-0.059894	4.815358
294.350924	7999.887574	14.070618	-0.059886	4.815357
294.218133	7999.961264	14.075623	-0.059861	4.815380
294.378466	7999.895517	14.080627	-0.059891	4.815360
294.283320	7999.880050	14.085632	-0.059873	4.815355
294.338316	7999.872413	14.090637	-0.059884	4.815353
294.491429	7999.780895	14.095642	-0.059912	4.815326
294.350451	7999.941022	14.100647	-0.059886	4.815373
294.295487	7999.859955	14.105651	-0.059876	4.815350
294.400350	7999.766570	14.110656	-0.059895	4.815322
294.329964	7999.959929	14.115661	-0.059882	4.815379
294.574463	7999.866717	14.120666	-0.059928	4.815350
294.401872	7999.859588	14.125671	-0.059896	4.815349
294.350722	7999.781790	14.130675	-0.059886	4.815326
294.440009	7999.879463	14.135680	-0.059903	4.815355
294.219029	7999.887564	14.140685	-0.059862	4.815358
294.335598	7999.780479	14.145690	-0.059883	4.815326
294.363577	7999.879274	14.150695	-0.059889	4.815355
294.222927	7999.967796	14.155699	-0.059863	4.815381
294.251397	7999.866734	14.160704	-0.059868	4.815352
294.149578	7999.968725	14.165709	-0.059849	4.815382
294.312242	7999.835682	14.170714	-0.059879	4.815342
294.186989	7999.926597	14.175719	-0.059856	4.815370
294.311050	7999.864525	14.180723	-0.059879	4.815351
294.297553	7999.874992	14.185728	-0.059877	4.815354
294.398703	7999.876669	14.190733	-0.059895	4.815354
294.531024	7999.797633	14.195738	-0.059920	4.815330
294.354945	7999.866331	14.200743	-0.059887	4.815351
294.335040	7999.888448	14.205747	-0.059884	4.815358
294.576216	7999.861448	14.210752	-0.059929	4.815349
294.367096	7999.886847	14.215757	-0.059890	4.815357
294.415740	7999.777568	14.220762	-0.059899	4.815325
294.342286	7999.867202	14.225767	-0.059885	4.815351
294.423440	7999.863204	14.230771	-0.059900	4.815350
294.317670	7999.859319	14.235776	-0.059881	4.815349
294.224283	7999.865257	14.240781	-0.059863	4.815351
294.329423	7999.887307	14.245786	-0.059883	4.815357
294.266769	7999.862759	14.250791	-0.059871	4.815350
294.167128	7999.873938	14.255795	-0.059853	4.815354
294.057656	7999.535462	14.260800	-0.059832	4.815256
294.122835	7996.311301	14.265805	-0.059842	4.814314
294.139487	7990.761325	14.270810	-0.059842	4.812692
294.130043	7983.954927	14.275815	-0.059835	4.810702
294.138597	7976.654281	14.280819	-0.059832	4.808567
294.022017	7969.012461	14.285824	-0.059806	4.806332
293.786047	7961.154863	14.290829	-0.059757	4.804033
294.100300	7953.370356	14.295834	-0.059810	4.801751
293.931242	7945.377550	14.300839	-0.059773	4.799410
293.606912	7937.442812	14.305843	-0.059708	4.797086
293.710776	7929.453491	14.310848	-0.059722	4.794742
293.692517	7921.363081	14.315853	-0.059713	4.792368
293.801103	7913.394412	14.320858	-0.059728	4.790028
293.694020	7905.367021	14.325863	-0.059703	4.787670
293.884061	7897.366931	14.330867	-0.059734	4.785319
293.886434	7889.437109	14.335872	-0.059729	4.782987
293.504424	7881.410407	14.340877	-0.059653	4.780628
293.772145	7873.454915	14.345882	-0.059697	4.778285
293.843244	7865.410516	14.350887	-0.059705	4.775916
293.716631	7857.379154	14.355891	-0.059676	4.773551
293.630879	7849.342827	14.360896	-0.059655	4.771182
293.686617	7841.375836	14.365901	-0.059660	4.768833
293.713413	7833.361617	14.370906	-0.059660	4.766468
293.550312	7825.365951	14.375911	-0.059625	4.764108
293.550814	7817.379472	14.380915	-0.059620	4.761750
293.588659	7809.397405	14.385920	-0.059622	4.759391
293.358437	7801.431977	14.390925	-0.059573	4.757037
293.733991	7793.341456	14.395930	-0.059638	4.754643
293.751562	7785.290889	14.400935	-0.059636	4.752260
293.362559	7777.233499	14.405939	-0.059559	4.749876
293.425025	7769.372818	14.410944	-0.059565	4.747547
293.226413	7761.305693	14.415949	-0.059523	4.745157
293.233544	7753.371209	14.420954	-0.059519	4.742805
293.168673	7745.342075	14.425959	-0.059502	4.740423
293.206762	7737.320162	14.430963	-0.059504	4.738042
293.341124	7729.367352	14.435968	-0.059524	4.735679
293.224526	7721.274187	14.440973	-0.059497	4.733275
293.316187	7713.313187	14.445978	-0.059509	4.730908
293.179204	7705.333001	14.450983	-0.059478	4.728535
292.974282	7697.272342	14.455987	-0.059434	4.726137
293.168767	7689.320113	14.460992	-0.059466	4.723769
293.109242	7681.312977	14.465997	-0.059449	4.721384
293.162142	7673.258524	14.471002	-0.059454	4.718984
293.032486	7665.340604	14.476007	-0.059425	4.716623
292.875539	7657.315576	14.481011	-0.059390	4.714230
292.824217	7649.285088	14.486016	-0.059375	4.711833
292.693778	7641.246594	14.491021	-0.059346	4.709433
292.746360	7633.305592	14.496026	-0.059351	4.707060
292.705395	7625.235278	14.501031	-0.059338	4.704648
292.536988	7617.325781	14.506035	-0.059301	4.702282
292.821596	7609.291081	14.511040	-0.059349	4.699878
292.710554	7601.317086	14.516045	-0.059323	4.697491
292.814753	7593.306960	14.521050	-0.059337	4.695091
292.598102	7585.273813	14.526055	-0.059292	4.692684
292.896611	7577.234603	14.531059	-0.059342	4.690273
292.729402	7569.304768	14.536064	-0.059306	4.687894
292.621924	7561.218207	14.541069	-0.059281	4.685467
292.685726	7553.312514	14.546074	-0.059287	4.683093
292.620272	7545.292713	14.551079	-0.059270	4.680683
292.454827	7537.330530	14.556083	-0.059234	4.678290
292.403475	7529.278650	14.561088	-0.059219	4.675868
292.260796	7521.181770	14.566093	-0.059187	4.673432
292.365894	7513.169140	14.571098	-0.059202	4.671019
292.254323	7505.174133	14.576103	-0.059176	4.668611
292.478485	7497.178560	14.581107	-0.059212	4.666201
292.472313	7489.257493	14.586112	-0.059206	4.663812
292.426900	7481.237923	14.591117	-0.059192	4.661392
292.233350	7473.236456	14.596122	-0.059151	4.658977
292.223775	7465.269853	14.601127	-0.059144	4.656571
292.074249	7457.182957	14.606131	-0.059111	4.654127
292.050625	7449.232919	14.611136	-0.059102	4.651724
292.002019	7441.160021	14.616141	-0.059087	4.649282
292.030575	7433.242172	14.621146	-0.059088	4.646885
292.169246	7425.218409	14.626151	-0.059108	4.644455
291.959335	7417.213401	14.631155	-0.059064	4.642030
292.061173	7409.181448	14.636160	-0.059078	4.639595
291.931818	7401.237591	14.641165	-0.059048	4.637186
291.967345	7393.236515	14.646170	-0.059050	4.634758
291.962748	7385.157318	14.651175	-0.059044	4.632305
292.000940	7377.135902	14.656179	-0.059046	4.629869
291.896303	7369.218132	14.661184	-0.059021	4.627462
291.869735	7361.158867	14.666189	-0.059011	4.625011
291.957474	7353.240432	14.671194	-0.059022	4.622602
291.746031	7345.209005	14.676199	-0.058978	4.620157
291.471195	7337.198283	14.681203	-0.058921	4.617717
291.645332	7329.161324	14.686208	-0.058948	4.615268
291.813935	7321.156211	14.691213	-0.058975	4.612827
291.708241	7313.151206	14.696218	-0.058950	4.610385
291.680727	7305.152516	14.701223	-0.058939	4.607944
291.707661	7297.114111	14.706227	-0.058939	4.605489
291.722153	7289.209728	14.711232	-0.058937	4.603074
291.448965	7281.177017	14.716237	-0.058881	4.600618
291.761227	7273.198098	14.721242	-0.058934	4.598178
291.416745	7265.175161	14.726247	-0.058864	4.595722
291.448797	7257.081706	14.731251	-0.058865	4.593244
291.373206	7249.098741	14.736256	-0.058846	4.590798
291.120438	7241.115299	14.741261	-0.058794	4.588351
291.204754	7233.112138	14.746266	-0.058804	4.585896
291.287529	7225.137651	14.751271	-0.058814	4.583449
291.197991	7217.120034	14.756275	-0.058792	4.580988
291.170229	7209.147251	14.761280	-0.058782	4.578538
291.028805	7201.133374	14.766285	-0.058751	4.576075
291.132608	7193.108934	14.771290	-0.058765	4.573608
291.082323	7185.133916	14.776295	-0.058750	4.571154
291.009532	7177.077108	14.781299	-0.058731	4.568673
291.168460	7169.119134	14.786304	-0.058756	4.566222
290.906176	7161.084931	14.791309	-0.058702	4.563746
290.988623	7153.121654	14.796314	-0.058712	4.561290
291.035995	7145.127379	14.801319	-0.058716	4.558824
290.758977	7137.156015	14.806323	-0.058659	4.556363
290.704825	7129.155728	14.811328	-0.058644	4.553892
290.692651	7121.092956	14.816333	-0.058636	4.551400
290.784574	7113.094665	14.821338	-0.058648	4.548927
290.844374	7105.104896	14.826343	-0.058654	4.546455
290.673236	7097.092449	14.831347	-0.058617	4.543975
290.536333	7089.141707	14.836352	-0.058586	4.541512
290.529300	7081.099921	14.841357	-0.058580	4.539020
290.490855	7073.140261	14.846362	-0.058567	4.536553
290.377107	7065.115991	14.851367	-0.058541	4.534063
290.372768	7057.060300	14.856371	-0.058535	4.531563
290.497897	7049.110738	14.861376	-0.058553	4.529094
290.330809	7041.063958	14.866381	-0.058517	4.526593
290.378705	7033.099532	14.871386	-0.058521	4.524117
290.266979	7025.111484	14.876391	-0.058495	4.521632
290.317871	7017.106645	14.881395	-0.058499	4.519141
290.329862	7009.153604	14.886400	-0.058496	4.516664
290.389361	7001.092377	14.891405	-0.058502	4.514152
290.301687	6993.043782	14.896410	-0.058480	4.511643
290.245818	6985.047479	14.901415	-0.058465	4.509148
290.371285	6977.031142	14.906419	-0.058483	4.506647
290.364327	6969.080296	14.911424	-0.058476	4.504164
290.164782	6961.047597	14.916429	-0.058434	4.501654
290.236446	6953.088962	14.921434	-0.058442	4.499166
290.135033	6945.058437	14.926439	-0.058418	4.496653
289.854732	6937.037082	14.931443	-0.058361	4.494142
289.933635	6929.015965	14.936448	-0.058370	4.491630
289.838101	6921.049790	14.941453	-0.058347	4.489134
289.836746	6913.047350	14.946458	-0.058342	4.486625
289.678698	6905.059911	14.951463	-0.058307	4.484119
289.805643	6897.048258	14.956467	-0.058326	4.481605
289.846301	6889.070775	14.961472	-0.058328	4.479100
289.622403	6881.064776	14.966477	-0.058281	4.476584
289.838683	6873.030853	14.971482	-0.058316	4.474058
289.558309	6864.992925	14.976487	-0.058259	4.471529
289.575465	6857.038660	14.981491	-0.058257	4.469025
289.538018	6849.026043	14.986496	-0.058245	4.466502
289.617634	6840.995830	14.991501	-0.058254	4.463972
289.680441	6833.022810	14.996506	-0.058261	4.461458
289.496140	6825.013673	15.001511	-0.058221	4.458931
289.590456	6817.027544	15.006515	-0.058234	4.456411
289.516811	6809.020295	15.011520	-0.058215	4.453882
289.302819	6800.975924	15.016525	-0.058170	4.451339
289.420106	6792.976466	15.021530	-0.058187	4.448810
289.311099	6784.982456	15.026535	-0.058161	4.446280
289.357924	6776.987067	15.031539	-0.058165	4.443750
289.395454	6769.057444	15.036544	-0.058166	4.441238
289.429043	6761.019090	15.041549	-0.058167	4.438691
289.434102	6753.047747	15.046554	-0.058163	4.436164
289.273907	6744.992733	15.051559	-0.058128	4.433607
289.226184	6736.936927	15.056563	-0.058114	4.431050
289.331743	6728.957315	15.061568	-0.058129	4.428516
289.193206	6720.934688	15.066573	-0.058098	4.425965
289.161431	6712.978004	15.071578	-0.058087	4.423435
289.176338	6705.007546	15.076583	-0.058084	4.420899
289.054412	6696.999599	15.081587	-0.058056	4.418349
288.982958	6688.979889	15.086592	-0.058038	4.415794
288.797076	6680.950950	15.091597	-0.057998	4.413234
288.946433	6672.943060	15.096602	-0.058021	4.410681
288.915576	6664.956291	15.101607	-0.058010	4.408132
288.864036	6656.920729	15.106611	-0.057995	4.405566
289.009646	6648.995131	15.111616	-0.058017	4.403034
288.748516	6640.938142	15.116621	-0.057963	4.400458
288.714541	6632.996393	15.121626	-0.057951	4.397917
288.647899	6625.009090	15.126631	-0.057934	4.395361
288.614819	6616.939157	15.131635	-0.057922	4.392776
288.530227	6608.952802	15.136640	-0.057902	4.390217
288.371660	6600.926672	15.141645	-0.057867	4.387643
288.635819	6592.948513	15.146650	-0.057911	4.385085
288.554543	6584.995614	15.151655	-0.057891	4.382532
288.429562	6576.947105	15.156659	-0.057862	4.379946
288.608522	6569.059131	15.161664	-0.057890	4.377412
288.575611	6560.963078	15.166669	-0.057879	4.374809
288.443527	6552.975556	15.171674	-0.057849	4.372238
288.534901	6544.946931	15.176679	-0.057861	4.369654
288.294255	6536.972893	15.181683	-0.057811	4.367084
288.417087	6528.968643	15.186688	-0.057829	4.364505
288.442756	6521.014504	15.191693	-0.057828	4.361940
288.562207	6512.973267	15.196698	-0.057845	4.359346
288.098760	6505.032322	15.201703	-0.057754	4.356779
288.072317	6496.944606	15.206707	-0.057744	4.354166
288.171052	6488.878566	15.211712	-0.057757	4.351559
288.036544	6480.879939	15.216717	-0.057727	4.348971
288.095202	6472.916906	15.221722	-0.057732	4.346394
288.195938	6464.930729	15.226727	-0.057746	4.343808
287.985242	6456.940342	15.231731	-0.057702	4.341218
288.085892	6448.993522	15.236736	-0.057715	4.338642
287.839091	6440.944271	15.241741	-0.057664	4.336028
287.918673	6432.961262	15.246746	-0.057674	4.333437
287.756851	6424.929601	15.251751	-0.057638	4.330828
287.639152	6416.941264	15.256755	-0.057611	4.328230
287.738748	6408.921334	15.261760	-0.057625	4.325623
287.818057	6400.956532	15.266765	-0.057634	4.323032
287.963978	6392.942273	15.271770	-0.057656	4.320423
287.758448	6384.995330	15.276775	-0.057613	4.317832
287.801905	6376.906851	15.281779	-0.057616	4.315196
287.707657	6368.932668	15.286784	-0.057593	4.312594
287.459057	6360.888503	15.291789	-0.057541	4.309967
287.744644	6352.925767	15.296794	-0.057589	4.307368
287.769188	6344.896508	15.301799	-0.057589	4.304744
287.573368	6336.937498	15.306803	-0.057547	4.302140
287.709014	6328.917284	15.311808	-0.057567	4.299517
287.391967	6320.945237	15.316813	-0.057503	4.296905
287.359572	6312.926483	15.321818	-0.057492	4.294278
287.172646	6304.896446	15.326823	-0.057452	4.291644
287.383190	6296.892062	15.331827	-0.057486	4.289020
287.358365	6288.925931	15.336832	-0.057476	4.286405
287.172339	6280.863227	15.341837	-0.057436	4.283756
287.311412	6272.934151	15.346842	-0.057457	4.281152
287.520314	6264.919799	15.351847	-0.057491	4.278518
287.175732	6256.933036	15.356851	-0.057421	4.275888
287.284129	6248.883697	15.361856	-0.057436	4.273239
287.206699	6240.842255	15.366861	-0.057417	4.270589
287.067605	6232.881316	15.371866	-0.057385	4.267964
286.903640	6224.818121	15.376871	-0.057350	4.265303
286.994753	6216.894149	15.381875	-0.057362	4.262689
287.043336	6208.905267	15.386880	-0.057365	4.260051
286.942155	6200.935754	15.391885	-0.057341	4.257416
286.974836	6192.872247	15.396890	-0.057342	4.254751
286.874789	6184.900436	15.401895	-0.057318	4.252112
286.925781	6176.874776	15.406899	-0.057323	4.249456
286.945761	6168.936951	15.411904	-0.057321	4.246826
286.652298	6160.896053	15.416909	-0.057261	4.244158
286.598488	6152.947686	15.421914	-0.057246	4.241521
286.664731	6144.928478	15.426919	-0.057253	4.238860
286.673665	6136.920621	15.431923	-0.057250	4.236201
286.668927	6128.911616	15.436928	-0.057244	4.233540
286.411811	6120.837995	15.441933	-0.057191	4.230853
286.618826	6112.891167	15.446938	-0.057224	4.228210
286.671281	6104.904079	15.451943	-0.057229	4.225552
286.463847	6096.917497	15.456947	-0.057185	4.222889
286.617910	6088.919686	15.461952	-0.057208	4.220224
286.571776	6080.933795	15.466957	-0.057195	4.217560
286.451394	6072.933704	15.471962	-0.057167	4.214888
286.416314	6064.918404	15.476967	-0.057155	4.212211
286.509474	6056.910850	15.481971	-0.057167	4.209536
286.571097	6048.954120	15.486976	-0.057174	4.206876
286.513084	6040.919361	15.491981	-0.057158	4.204186
286.450176	6032.957967	15.496986	-0.057141	4.201520
286.309455	6024.945410	15.501991	-0.057110	4.198834
286.176294	6016.913605	15.506995	-0.057080	4.196139
286.138985	6008.861661	15.512000	-0.057067	4.193438
286.171096	6000.766236	15.517005	-0.057068	4.190720
286.024215	5992.836944	15.522010	-0.057036	4.188055
285.916614	5984.867863	15.527015	-0.057010	4.185375
286.084249	5976.899652	15.532019	-0.057036	4.182697
286.036514	5968.922182	15.537024	-0.057022	4.180011
285.822781	5960.923805	15.542029	-0.056977	4.177315
285.898414	5952.916506	15.547034	-0.056986	4.174617
286.039954	5944.896439	15.552039	-0.057007	4.171914
285.737636	5936.870443	15.557043	-0.056946	4.169202
285.776771	5928.886396	15.562048	-0.056948	4.166507
285.805620	5920.877373	15.567053	-0.056948	4.163801
285.747735	5912.925421	15.572058	-0.056932	4.161112
285.593765	5904.910893	15.577063	-0.056898	4.158398
285.759962	5896.844574	15.582067	-0.056924	4.155669
285.737770	5888.874758	15.587072	-0.056915	4.152969
285.484130	5880.833483	15.592077	-0.056862	4.150240
285.685891	5872.860821	15.597082	-0.056895	4.147538
285.534243	5864.893743	15.602087	-0.056861	4.144832
285.546050	5856.888491	15.607091	-0.056858	4.142113
285.762832	5848.883054	15.612096	-0.056894	4.139395
285.674727	5840.882671	15.617101	-0.056872	4.136673
285.420576	5832.882555	15.622106	-0.056820	4.133947
285.397739	5824.857484	15.627111	-0.056810	4.131214
285.461573	5816.845584	15.632115	-0.056817	4.128484
285.549385	5808.876529	15.637120	-0.056828	4.125767
285.251049	5800.903077	15.642125	-0.056767	4.123043
285.346745	5792.851947	15.647130	-0.056780	4.120295
285.389827	5784.923193	15.652135	-0.056783	4.117586
285.111035	5776.874723	15.657139	-0.056726	4.114831
285.165981	5768.879468	15.662144	-0.056731	4.112096
285.071133	5760.822233	15.667149	-0.056708	4.109336
285.238221	5752.830687	15.672154	-0.056734	4.106600
284.971127	5744.868203	15.677159	-0.056679	4.103867
284.799267	5736.860195	15.682163	-0.056642	4.101117
285.088496	5728.889919	15.687168	-0.056690	4.098385
284.917831	5720.877195	15.692173	-0.056653	4.095630
284.896884	5712.895905	15.697178	-0.056644	4.092886
284.880155	5704.877177	15.702183	-0.056636	4.090128
284.692060	5696.904136	15.707187	-0.056596	4.087381
284.707995	5688.886826	15.712192	-0.056594	4.084619
284.685719	5680.926250	15.717197	-0.056584	4.081875
284.693249	5672.930045	15.722202	-0.056580	4.079117
284.488875	5664.945011	15.727207	-0.056537	4.076358
284.541337	5656.910882	15.732211	-0.056542	4.073584
284.793060	5648.900356	15.737216	-0.056583	4.070819
284.752608	5640.885368	15.742221	-0.056571	4.068046
284.566950	5632.889901	15.747226	-0.056531	4.065276
284.700551	5624.937360	15.752231	-0.056551	4.062524
284.464015	5616.904527	15.757235	-0.056501	4.059736
284.353874	5608.980081	15.762240	-0.056476	4.056987
284.274969	5600.948253	15.767245	-0.056456	4.054198
284.604504	5592.877094	15.772250	-0.056512	4.051400
284.627483	5584.935587	15.777255	-0.056511	4.048640
284.322077	5576.916394	15.782259	-0.056449	4.045847
284.297132	5568.954685	15.787264	-0.056439	4.043076
284.247212	5560.905414	15.792269	-0.056425	4.040272
284.192554	5552.959576	15.797274	-0.056409	4.037502
284.389846	5544.909081	15.802279	-0.056441	4.034698
284.272509	5536.787332	15.807283	-0.056414	4.031862
284.230495	5528.837003	15.812288	-0.056401	4.029085
283.923548	5520.868863	15.817293	-0.056339	4.026295
283.979086	5512.906621	15.822298	-0.056344	4.023512
283.882329	5504.915526	15.827303	-0.056321	4.020714
283.746054	5496.920196	15.832307	-0.056290	4.017912
283.959174	5488.875868	15.837312	-0.056324	4.015096
283.901269	5480.862491	15.842317	-0.056308	4.012285
284.062097	5472.877906	15.847322	-0.056333	4.009486
283.905459	5464.921951	15.852327	-0.056299	4.006689
283.803314	5456.891020	15.857331	-0.056275	4.003865
283.702467	5448.923429	15.862336	-0.056251	4.001062
283.768317	5440.889168	15.867341	-0.056258	3.998236
283.768538	5432.907868	15.872346	-0.056253	3.995425
283.897153	5424.897977	15.877351	-0.056271	3.992604
283.557888	5416.866536	15.882355	-0.056203	3.989766
283.616793	5408.915430	15.887360	-0.056209	3.986961
283.711147	5400.903750	15.892365	-0.056221	3.984133
283.744054	5392.910300	15.897370	-0.056222	3.981309
283.694184	5384.914030	15.902375	-0.056208	3.978480
283.506129	5376.892045	15.907379	-0.056168	3.975638
283.534235	5368.922971	15.912384	-0.056168	3.972816
283.579134	5360.841647	15.917389	-0.056171	3.969952
283.624262	5352.942113	15.922394	-0.056174	3.967151
283.417823	5344.925619	15.927399	-0.056130	3.964302
283.337077	5336.978372	15.932403	-0.056110	3.961478
283.412518	5328.966104	15.937408	-0.056119	3.958631
283.355003	5320.945815	15.942413	-0.056103	3.955778
283.163702	5312.930819	15.947418	-0.056062	3.952921
283.306575	5304.896674	15.952423	-0.056084	3.950062
283.158553	5296.934164	15.957427	-0.056051	3.947221
283.098142	5288.932915	15.962432	-0.056035	3.944365
282.819982	5280.973570	15.967437	-0.055978	3.941519
283.054924	5272.974632	15.972442	-0.056016	3.938666
283.076770	5264.967536	15.977447	-0.056015	3.935803
282.892590	5256.953851	15.982451	-0.055976	3.932933
282.887844	5248.977220	15.987456	-0.055969	3.930077
282.649769	5240.979791	15.992461	-0.055920	3.927207
282.656047	5232.967290	15.997466	-0.055916	3.924334
282.670025	5225.000280	16.002471	-0.055913	3.921476
282.735133	5216.960869	16.007475	-0.055920	3.918590
282.734550	5208.992372	16.012480	-0.055915	3.915727
282.540516	5200.979734	16.017485	-0.055874	3.912842
282.648151	5192.953256	16.022490	-0.055889	3.909955
282.734106	5184.990977	16.027495	-0.055899	3.907089
282.604769	5176.921834	16.032499	-0.055870	3.904178
282.559535	5168.985919	16.037504	-0.055857	3.901315
282.593857	5160.999827	16.042509	-0.055858	3.898433
282.364163	5153.003218	16.047514	-0.055810	3.895540
282.419562	5144.976088	16.052519	-0.055815	3.892640
282.607669	5136.929807	16.057523	-0.055845	3.889733
282.631686	5129.013671	16.062528	-0.055844	3.886867
282.352333	5120.983384	16.067533	-0.055787	3.883952
282.479069	5112.978913	16.072538	-0.055805	3.881053
282.269212	5105.025914	16.077543	-0.055761	3.878163
282.051964	5096.983936	16.082547	-0.055715	3.875239
282.202034	5088.772024	16.087552	-0.055738	3.872257
282.333903	5080.768169	16.092557	-0.055757	3.869349
282.364671	5072.869241	16.097562	-0.055758	3.866475
282.186778	5064.915571	16.102567	-0.055720	3.863575
282.016213	5056.934163	16.107571	-0.055683	3.860662
282.179716	5048.979027	16.112576	-0.055708	3.857764
282.024278	5040.942213	16.117581	-0.055674	3.854827
281.820128	5032.952732	16.122586	-0.055631	3.851904
281.905495	5024.971279	16.127591	-0.055641	3.848988
281.742279	5016.985796	16.132595	-0.055606	3.846063
281.777056	5008.997113	16.137600	-0.055607	3.843138
281.879680	5000.995370	16.142605	-0.055621	3.840208
281.817217	4993.056637	16.147610	-0.055604	3.837296
281.734826	4985.025595	16.152615	-0.055584	3.834347
281.849363	4977.003220	16.157619	-0.055600	3.831403
282.051672	4968.956510	16.162624	-0.055632	3.828449
281.695469	4960.974066	16.167629	-0.055561	3.825506
281.673748	4953.049159	16.172634	-0.055552	3.822588
281.800276	4945.066749	16.177639	-0.055570	3.819650
281.667230	4937.091837	16.182643	-0.055540	3.816707
281.503124	4929.046276	16.187648	-0.055504	3.813735
281.400771	4921.052502	16.192653	-0.055480	3.810780
281.523404	4913.037536	16.197658	-0.055498	3.807821
281.542720	4905.034783	16.202663	-0.055496	3.804862
281.614271	4897.085785	16.207667	-0.055504	3.801921
281.386789	4889.130992	16.212672	-0.055457	3.798970
281.170456	4881.104378	16.217677	-0.055411	3.795989
281.121556	4873.048192	16.222682	-0.055397	3.792999
281.426127	4865.005994	16.227687	-0.055448	3.790020
281.267208	4857.042933	16.232691	-0.055414	3.787058
281.085191	4849.062380	16.237696	-0.055375	3.784086
281.039779	4841.087547	16.242701	-0.055361	3.781117
281.019384	4833.083146	16.247706	-0.055352	3.778135
281.014760	4825.101711	16.252711	-0.055346	3.775160
280.984982	4817.038588	16.257715	-0.055335	3.772151
281.253541	4809.068299	16.262720	-0.055380	3.769181
281.089560	4801.069540	16.267725	-0.055344	3.766189
280.887519	4793.113756	16.272730	-0.055302	3.763209
281.072457	4785.104805	16.277735	-0.055331	3.760216
281.172603	4777.084871	16.282739	-0.055344	3.757215
280.864117	4769.107320	16.287744	-0.055282	3.754217
280.836287	4761.056536	16.292749	-0.055271	3.751196
280.925645	4753.072314	16.297754	-0.055283	3.748201
280.747377	4745.091162	16.302759	-0.055244	3.745198
280.501704	4737.109085	16.307763	-0.055193	3.742190
280.616104	4729.125919	16.312768	-0.055210	3.739189
280.594983	4721.112062	16.317773	-0.055200	3.736170
280.600573	4713.116260	16.322778	-0.055196	3.733156
280.617682	4705.122883	16.327783	-0.055194	3.730140
280.625561	4697.086962	16.332787	-0.055191	3.727106
280.522063	4689.120826	16.337792	-0.055166	3.724094
280.382083	4681.180844	16.342797	-0.055135	3.721088
280.479595	4673.180209	16.347802	-0.055148	3.718062
280.302908	4665.188814	16.352807	-0.055110	3.715030
280.405106	4657.084007	16.357811	-0.055124	3.711960
280.343457	4649.114880	16.362816	-0.055107	3.708935
280.286429	4641.090353	16.367821	-0.055091	3.705886
280.161689	4633.130231	16.372826	-0.055063	3.702858
280.210794	4625.157154	16.377831	-0.055067	3.699826
280.050301	4617.179695	16.382835	-0.055032	3.696786
279.931292	4609.191415	16.387840	-0.055004	3.693739
279.870665	4601.169937	16.392845	-0.054988	3.690679
279.775433	4593.222027	16.397850	-0.054965	3.687643
279.946769	4585.184652	16.402855	-0.054992	3.684578
279.833746	4577.222546	16.407859	-0.054965	3.681531
279.836152	4569.230862	16.412864	-0.054961	3.678474
279.730471	4561.214729	16.417869	-0.054936	3.675402
279.886289	4553.179721	16.422874	-0.054960	3.672327
279.989502	4545.181758	16.427879	-0.054974	3.669262
279.565705	4537.199868	16.432883	-0.054890	3.666187
279.681573	4529.224209	16.437888	-0.054906	3.663126
279.534659	4521.214510	16.442893	-0.054873	3.660042
279.606354	4513.254379	16.447898	-0.054882	3.656981
279.634526	4505.236599	16.452903	-0.054882	3.653894
279.389585	4497.194838	16.457907	-0.054831	3.650787
279.684654	4489.217729	16.462912	-0.054881	3.647717
279.792721	4481.202659	16.467917	-0.054896	3.644625
279.757753	4473.275249	16.472922	-0.054884	3.641561
279.737609	4465.281705	16.477927	-0.054875	3.638468
279.638802	4457.239954	16.482931	-0.054851	3.635353
279.495164	4449.252557	16.487936	-0.054819	3.632254
279.360083	4441.230408	16.492941	-0.054789	3.629140
279.495803	4433.218832	16.497946	-0.054809	3.626034
279.525056	4425.266502	16.502951	-0.054809	3.622946
279.272580	4417.244390	16.507955	-0.054757	3.619820
279.330733	4409.290879	16.512960	-0.054763	3.616726
279.371741	4401.266033	16.517965	-0.054765	3.613602
279.338820	4393.247741	16.522970	-0.054754	3.610476
279.403022	4385.295117	16.527975	-0.054761	3.607375
279.205257	4377.270436	16.532979	-0.054719	3.604236
279.062637	4369.381460	16.537984	-0.054687	3.601149
278.975666	4361.341359	16.542989	-0.054666	3.598002
278.941274	4353.346815	16.547994	-0.054654	3.594871
279.073252	4345.364020	16.552999	-0.054674	3.591747
278.860753	4337.319850	16.558003	-0.054629	3.588586
279.004896	4329.327052	16.563008	-0.054650	3.585453
278.888279	4321.366435	16.568013	-0.054624	3.582322
278.797089	4313.364162	16.573018	-0.054601	3.579173
278.621452	4305.417158	16.578023	-0.054564	3.576041
278.900352	4297.344174	16.583027	-0.054610	3.572869
278.891468	4289.374514	16.588032	-0.054603	3.569726
278.596822	4281.387000	16.593037	-0.054543	3.566566
278.750707	4273.387899	16.598042	-0.054567	3.563411
278.769031	4265.406615	16.603047	-0.054565	3.560257
278.665971	4257.435078	16.608051	-0.054541	3.557100
278.714295	4249.393241	16.613056	-0.054544	3.553916
278.694278	4241.295969	16.618061	-0.054536	3.550706
278.794130	4233.344972	16.623066	-0.054549	3.547555
278.490641	4225.391874	16.628071	-0.054487	3.544388
278.456267	4217.421920	16.633075	-0.054476	3.541220
278.385474	4209.430479	16.638080	-0.054457	3.538039
278.301648	4201.404921	16.643085	-0.054437	3.534841
278.217893	4193.411721	16.648090	-0.054416	3.531653
278.130663	4185.415876	16.653095	-0.054394	3.528461
278.012764	4177.424950	16.658099	-0.054367	3.525267
277.996744	4169.503070	16.663104	-0.054359	3.522101
278.145551	4161.472752	16.668109	-0.054382	3.518894
278.085190	4153.464922	16.673114	-0.054365	3.515686
277.946805	4145.473534	16.678119	-0.054334	3.512480
277.788577	4137.455247	16.683123	-0.054300	3.509259
277.854055	4129.467570	16.688128	-0.054307	3.506055
277.950576	4121.465354	16.693133	-0.054319	3.502843
277.999937	4113.486511	16.698138	-0.054323	3.499635
277.842807	4105.551163	16.703143	-0.054289	3.496436
277.661079	4097.518188	16.708147	-0.054250	3.493194
277.632606	4089.516387	16.713152	-0.054239	3.489966
277.652522	4081.566924	16.718157	-0.054238	3.486758
277.751464	4073.524343	16.723162	-0.054251	3.483512
277.754190	4065.560834	16.728167	-0.054247	3.480292
277.553260	4057.602257	16.733171	-0.054204	3.477064
277.590847	4049.581479	16.738176	-0.054206	3.473815
277.392421	4041.543802	16.743181	-0.054164	3.470549
277.403559	4033.557104	16.748186	-0.054161	3.467308
277.531261	4025.568594	16.753191	-0.054179	3.464066
277.202408	4017.594025	16.758195	-0.054113	3.460812
277.353528	4009.606338	16.763200	-0.054136	3.457566
277.454771	4001.587201	16.768205	-0.054149	3.454302
277.352734	3993.592711	16.773210	-0.054125	3.451038
277.126210	3985.611283	16.778215	-0.054078	3.447772
277.151393	3977.586643	16.783219	-0.054077	3.444494
277.414609	3969.645730	16.788224	-0.054121	3.441255
277.126765	3961.676112	16.793229	-0.054062	3.437983
277.285222	3953.605559	16.798234	-0.054087	3.434681
277.377255	3945.635607	16.803239	-0.054099	3.431415
277.113026	3937.633165	16.808243	-0.054044	3.428121
277.148864	3929.648123	16.813248	-0.054046	3.424841
277.013564	3921.688570	16.818253	-0.054015	3.421562
277.022282	3913.689995	16.823258	-0.054012	3.418269
276.861814	3905.705519	16.828263	-0.053977	3.414973
276.877221	3897.689322	16.833267	-0.053974	3.411666
276.949892	3889.697305	16.838272	-0.053983	3.408368
276.729800	3881.726755	16.843277	-0.053937	3.405066
276.842043	3873.753707	16.848282	-0.053952	3.401771
276.934312	3865.761373	16.853287	-0.053964	3.398464
276.761480	3857.768855	16.858291	-0.053927	3.395145
276.862735	3849.664242	16.863296	-0.053941	3.391786
276.889527	3841.673791	16.868301	-0.053940	3.388467
276.641540	3833.694052	16.873306	-0.053889	3.385141
276.560389	3825.772666	16.878311	-0.053869	3.381841
276.545704	3817.776276	16.883315	-0.053861	3.378510
276.582382	3809.805876	16.888320	-0.053863	3.375187
276.307008	3801.806307	16.893325	-0.053806	3.371838
276.295990	3793.787807	16.898330	-0.053799	3.368487
276.473233	3785.806722	16.903335	-0.053827	3.365155
276.134930	3777.852263	16.908339	-0.053759	3.361813
276.214800	3769.854357	16.913344	-0.053768	3.358464
276.174023	3761.857665	16.918349	-0.053755	3.355108
276.224304	3753.825480	16.923354	-0.053760	3.351737
276.120208	3745.835479	16.928359	-0.053735	3.348374
276.074928	3737.815094	16.933363	-0.053721	3.344998
276.246547	3729.884023	16.938368	-0.053748	3.341664
276.257463	3721.885957	16.943373	-0.053745	3.338292
275.867182	3713.909500	16.948378	-0.053667	3.334911
276.207015	3705.897480	16.953383	-0.053725	3.331539
276.014742	3697.897947	16.958387	-0.053684	3.328149
275.858765	3689.940330	16.963392	-0.053650	3.324774
275.585359	3681.984998	16.968397	-0.053594	3.321392
276.006468	3673.955359	16.973402	-0.053667	3.318002
275.760228	3665.977980	16.978407	-0.053616	3.314605
275.597744	3657.925876	16.983411	-0.053581	3.311176
275.728176	3649.928073	16.988416	-0.053600	3.307778
275.526236	3641.951133	16.993421	-0.053557	3.304373
275.448460	3634.008776	16.998426	-0.053538	3.300983
275.604429	3626.035469	17.003431	-0.053561	3.297586
275.520044	3617.997610	17.008435	-0.053540	3.294148
275.482759	3610.013569	17.013440	-0.053528	3.290732
275.268791	3602.052264	17.018445	-0.053483	3.287315
275.288747	3594.038961	17.023450	-0.053482	3.283881
275.310914	3586.075289	17.028455	-0.053481	3.280465
275.282005	3578.093285	17.033459	-0.053470	3.277035
275.396066	3570.079844	17.038464	-0.053486	3.273594
275.234994	3562.065698	17.043469	-0.053451	3.270138
274.991572	3554.091500	17.048474	-0.053401	3.266693
275.189039	3546.095743	17.053479	-0.053432	3.263252
275.257067	3538.090533	17.058483	-0.053440	3.259798
275.233075	3530.170789	17.063488	-0.053430	3.256374
274.933950	3522.131048	17.068493	-0.053369	3.252883
275.052427	3514.083278	17.073498	-0.053386	3.249402
275.102367	3506.156175	17.078503	-0.053390	3.245966
274.830293	3498.179498	17.083507	-0.053334	3.242493
275.000167	3490.177770	17.088512	-0.053361	3.239022
274.799293	3482.218216	17.093517	-0.053318	3.235551
274.728188	3474.151349	17.098522	-0.053300	3.232035
274.663553	3466.159256	17.103527	-0.053283	3.228549
274.667328	3458.135845	17.108531	-0.053278	3.225047
274.721950	3450.195665	17.113536	-0.053283	3.221580
274.780478	3442.210138	17.118541	-0.053289	3.218089
274.702031	3434.219750	17.123546	-0.053269	3.214588
274.639063	3426.260856	17.128551	-0.053252	3.211096
274.660110	3418.235178	17.133555	-0.053251	3.207575
274.566548	3410.266782	17.138560	-0.053228	3.204071
274.768297	3402.282733	17.143565	-0.053261	3.200568
274.504624	3394.345826	17.148570	-0.053206	3.197062
274.528995	3386.343643	17.153575	-0.053206	3.193536
274.531665	3378.291542	17.158579	-0.053201	3.189984
274.400495	3370.349488	17.163584	-0.053172	3.186470
274.202908	3362.378869	17.168589	-0.053130	3.182937
274.342985	3354.365098	17.173594	-0.053150	3.179395
274.332557	3346.417592	17.178599	-0.053143	3.175872
274.067874	3338.395088	17.183603	-0.053089	3.172301
274.110691	3330.392134	17.188608	-0.053092	3.168748
274.116070	3322.396845	17.193613	-0.053087	3.165192
273.998841	3314.453949	17.198618	-0.053060	3.161651
274.040221	3306.464722	17.203623	-0.053063	3.158092
274.003245	3298.452242	17.208627	-0.053051	3.154515
273.881083	3290.459265	17.213632	-0.053023	3.150939
273.957271	3282.450485	17.218637	-0.053032	3.147361
273.972425	3274.461625	17.223642	-0.053030	3.143785
273.911324	3266.508117	17.228647	-0.053013	3.140217
273.756284	3258.529797	17.233651	-0.052979	3.136630
273.690982	3250.533798	17.238656	-0.052962	3.133034
273.821131	3242.504857	17.243661	-0.052981	3.129429
273.815443	3234.527623	17.248666	-0.052975	3.125836
273.586716	3226.606552	17.253671	-0.052927	3.122255
273.526632	3218.601922	17.258675	-0.052910	3.118639
273.648127	3210.620333	17.263680	-0.052928	3.115038
273.500374	3202.625746	17.268685	-0.052895	3.111415
273.607104	3194.595881	17.273690	-0.052910	3.107783
273.660342	3186.632304	17.278695	-0.052915	3.104174
273.371774	3178.659948	17.283699	-0.052856	3.100541
273.365017	3170.688724	17.288704	-0.052849	3.096918
273.330123	3162.695379	17.293709	-0.052838	3.093279
273.127811	3154.667366	17.298714	-0.052795	3.089612
273.185553	3146.726727	17.303719	-0.052800	3.085993
273.128002	3138.731874	17.308723	-0.052784	3.082339
273.217907	3130.756167	17.313728	-0.052796	3.078697
273.317788	3122.767031	17.318733	-0.052809	3.075044
272.906446	3114.714722	17.323738	-0.052728	3.071335
273.101651	3106.721412	17.328743	-0.052759	3.067676
272.928083	3098.729668	17.333747	-0.052721	3.063996
272.876996	3090.789361	17.338752	-0.052707	3.060342
273.017968	3082.819245	17.343757	-0.052728	3.056678
272.870244	3074.831397	17.348762	-0.052695	3.052988
272.880505	3066.841096	17.353767	-0.052692	3.049300
272.673605	3058.866627	17.358771	-0.052648	3.045605
272.784250	3050.900863	17.363776	-0.052664	3.041924
272.675944	3042.930958	17.368781	-0.052638	3.038226
272.462683	3034.939983	17.373786	-0.052593	3.034509
272.786184	3026.908580	17.378791	-0.052648	3.030795
272.663818	3018.913759	17.383795	-0.052620	3.027071
272.819993	3010.934003	17.388800	-0.052644	3.023363
272.712294	3002.947989	17.393805	-0.052619	3.019635
272.615768	2995.018190	17.398810	-0.052596	3.015929
272.555715	2987.019589	17.403815	-0.052580	3.012189
272.606400	2979.006667	17.408819	-0.052584	3.008442
272.708662	2971.033578	17.413824	-0.052598	3.004712
272.512524	2963.097776	17.418829	-0.052556	3.000980
272.366592	2955.129449	17.423834	-0.052524	2.997230
272.380932	2947.119062	17.428839	-0.052521	2.993464
272.158865	2939.091435	17.433843	-0.052475	2.989673
272.179413	2931.118520	17.438848	-0.052473	2.985916
272.168760	2923.137796	17.443853	-0.052466	2.982148
272.116165	2915.164370	17.448858	-0.052451	2.978377
272.134340	2907.188247	17.453863	-0.052449	2.974604
271.815286	2899.198356	17.458867	-0.052385	2.970802
272.040893	2891.186853	17.463872	-0.052422	2.967012
271.963673	2883.212695	17.468877	-0.052402	2.963220
271.832976	2875.247972	17.473882	-0.052373	2.959425
271.918029	2867.288654	17.478887	-0.052383	2.955639
271.900271	2859.272068	17.483891	-0.052375	2.951815
271.792393	2851.299792	17.488896	-0.052349	2.948003
271.625933	2843.305725	17.493901	-0.052313	2.944172
271.892135	2835.312392	17.498906	-0.052358	2.940359
271.786273	2827.385317	17.503911	-0.052333	2.936554
271.678120	2819.371971	17.508915	-0.052307	2.932702
271.805021	2811.350084	17.513920	-0.052326	2.928853
271.692131	2803.387547	17.518925	-0.052300	2.925015
271.553053	2795.451982	17.523930	-0.052269	2.921184
271.584772	2787.483618	17.528935	-0.052269	2.917340
271.605548	2779.445575	17.533939	-0.052268	2.913458
271.521604	2771.409115	17.538944	-0.052247	2.909565
271.263683	2763.445768	17.543949	-0.052194	2.905694
271.359580	2755.486931	17.548954	-0.052207	2.901838
271.297964	2747.545755	17.553959	-0.052190	2.897977
271.170310	2739.542328	17.558963	-0.052161	2.894078
271.228735	2731.541288	17.563968	-0.052167	2.890184
271.035152	2723.594354	17.568973	-0.052126	2.886298
271.061334	2715.598629	17.573978	-0.052125	2.882394
271.052385	2707.639968	17.578983	-0.052119	2.878502
270.990002	2699.655997	17.583987	-0.052102	2.874589
270.867910	2691.665434	17.588992	-0.052074	2.870664
270.963923	2683.681117	17.593997	-0.052087	2.866748
270.852085	2675.694826	17.599002	-0.052061	2.862815
270.983088	2667.743583	17.604007	-0.052080	2.858907
270.674293	2659.779287	17.609011	-0.052017	2.854963
270.737099	2651.769065	17.614016	-0.052024	2.851012
270.759355	2643.794689	17.619021	-0.052023	2.847070
270.546514	2635.825829	17.624026	-0.051978	2.843113
270.666510	2627.868181	17.629031	-0.051995	2.839174
270.611611	2619.864094	17.634035	-0.051980	2.835197
270.536864	2611.872271	17.639040	-0.051961	2.831219
270.402745	2603.889717	17.644045	-0.051930	2.827237
270.357576	2595.897687	17.649050	-0.051917	2.823250
270.500184	2587.924233	17.654055	-0.051938	2.819277
270.344295	2579.971186	17.659059	-0.051904	2.815291
270.263492	2571.987846	17.664064	-0.051884	2.811289
270.268328	2563.997984	17.669069	-0.051879	2.807283
270.125690	2556.024082	17.674074	-0.051848	2.803271
270.140660	2548.073272	17.679079	-0.051845	2.799273
270.062813	2540.091258	17.684083	-0.051826	2.795249
270.182212	2532.064547	17.689088	-0.051843	2.791208
270.050700	2524.108133	17.694093	-0.051813	2.787182
270.193701	2516.127090	17.699098	-0.051835	2.783153
270.315332	2508.158776	17.704103	-0.051852	2.779124
270.014155	2500.211236	17.709107	-0.051791	2.775075
270.102409	2492.198079	17.714112	-0.051802	2.771010
270.050622	2484.233237	17.719117	-0.051787	2.766954
270.054503	2476.269296	17.724122	-0.051783	2.762897
270.154646	2468.317376	17.729127	-0.051796	2.758846
269.963902	2460.345317	17.734131	-0.051756	2.754761
269.818389	2452.287208	17.739136	-0.051723	2.750628
269.875450	2444.301411	17.744141	-0.051729	2.746538
269.832598	2436.336231	17.749146	-0.051716	2.742447
269.803360	2428.395913	17.754151	-0.051705	2.738364
269.703234	2420.424345	17.759155	-0.051681	2.734254
269.745421	2412.406791	17.764160	-0.051684	2.730122
269.809661	2404.450682	17.769165	-0.051691	2.726018
269.601897	2396.498476	17.774170	-0.051647	2.721892
269.525301	2388.563283	17.779175	-0.051627	2.717778
269.484264	2380.558325	17.784179	-0.051615	2.713623
269.321934	2372.566945	17.789184	-0.051579	2.709461
269.239027	2364.608396	17.794189	-0.051559	2.705314
269.246282	2356.630923	17.799194	-0.051555	2.701157
269.387637	2348.656183	17.804199	-0.051576	2.697004
269.238305	2340.686265	17.809203	-0.051543	2.692828
269.061612	2332.718982	17.814208	-0.051505	2.688646
269.003617	2324.746293	17.819213	-0.051489	2.684461
268.813506	2316.810360	17.824218	-0.051448	2.680281
268.933254	2308.826248	17.829223	-0.051465	2.676089
268.761262	2300.818330	17.834227	-0.051428	2.671859
268.949207	2292.826148	17.839232	-0.051458	2.667654
268.910742	2284.849818	17.844237	-0.051446	2.663435
268.948860	2276.872091	17.849242	-0.051448	2.659215
268.971988	2268.932959	17.854247	-0.051447	2.655007
268.774497	2260.934983	17.859251	-0.051405	2.650747
268.923073	2252.963009	17.864256	-0.051427	2.646516
268.737652	2245.011879	17.869261	-0.051388	2.642268
268.652356	2237.062214	17.874266	-0.051367	2.638020
268.624585	2229.084467	17.879271	-0.051356	2.633755
268.490960	2221.080555	17.884275	-0.051326	2.629461
268.604015	2213.122457	17.889280	-0.051342	2.625201
268.500567	2205.171741	17.894285	-0.051318	2.620924
268.451260	2197.201843	17.899290	-0.051303	2.616633
268.422372	2189.228906	17.904295	-0.051293	2.612335
268.266246	2181.246478	17.909299	-0.051259	2.608016
268.296495	2173.286483	17.914304	-0.051259	2.603714
268.242975	2165.329898	17.919309	-0.051244	2.599402
268.286391	2157.350582	17.924314	-0.051247	2.595077
268.235701	2149.199388	17.929319	-0.051232	2.590644
268.008007	2141.259987	17.934323	-0.051185	2.586307
268.193075	2133.311174	17.939328	-0.051214	2.581986
268.086875	2125.390995	17.944333	-0.051189	2.577654
267.902607	2117.439837	17.949338	-0.051150	2.573292
267.953076	2109.466153	17.954343	-0.051154	2.568926
267.907631	2101.493083	17.959347	-0.051140	2.564546
267.790848	2093.580113	17.964352	-0.051113	2.560187
267.875277	2085.604534	17.969357	-0.051124	2.555800
267.827522	2077.617790	17.974362	-0.051110	2.551391
267.968438	2069.626293	17.979367	-0.051131	2.546984
267.724162	2061.678908	17.984371	-0.051080	2.542567
267.765142	2053.751906	17.989376	-0.051083	2.538173
267.589569	2045.786482	17.994381	-0.051045	2.533735
267.505364	2037.794583	17.999386	-0.051024	2.529282
267.487650	2029.840195	18.004391	-0.051016	2.524845
267.486908	2021.872206	18.009395	-0.051010	2.520395
267.331325	2013.944278	18.014400	-0.050976	2.515948
267.375038	2005.924716	18.019405	-0.050979	2.511457
267.488196	1997.922200	18.024410	-0.050995	2.506971
267.334178	1989.996080	18.029415	-0.050961	2.502502
267.345756	1982.033780	18.034419	-0.050958	2.498016
267.365688	1974.064800	18.039424	-0.050957	2.493519
267.238059	1966.106662	18.044429	-0.050928	2.489008
267.051982	1958.148301	18.049434	-0.050888	2.484486
267.209117	1950.201202	18.054439	-0.050912	2.479986
267.234482	1942.221647	18.059443	-0.050912	2.475451
266.983062	1934.272200	18.064448	-0.050860	2.470903
267.157087	1926.282336	18.069453	-0.050887	2.466356
267.096963	1918.334121	18.074458	-0.050870	2.461807
266.880389	1910.413737	18.079463	-0.050825	2.457254
267.043831	1902.408667	18.084467	-0.050850	2.452672
266.964746	1894.443474	18.089472	-0.050830	2.448086
266.918711	1886.496758	18.094477	-0.050817	2.443504
266.782592	1878.554119	18.099482	-0.050786	2.438910
266.784830	1870.602905	18.104487	-0.050781	2.434312
266.649478	1862.538420	18.109491	-0.050751	2.429630
266.742137	1854.576840	18.114496	-0.050763	2.425015
266.607901	1846.657418	18.119501	-0.050733	2.420399
266.560647	1838.699904	18.124506	-0.050719	2.415759
266.738111	1830.722806	18.129511	-0.050747	2.411116
266.472786	1822.779004	18.134515	-0.050692	2.406448
266.411374	1814.839337	18.139520	-0.050676	2.401790
266.561882	1806.884470	18.144525	-0.050699	2.397131
266.316346	1798.937919	18.149530	-0.050648	2.392436
266.268239	1790.969354	18.154535	-0.050634	2.387735
266.166774	1783.013615	18.159539	-0.050610	2.383027
266.198198	1775.054785	18.164544	-0.050610	2.378319
265.917833	1767.126452	18.169549	-0.050553	2.373595
265.968870	1759.125438	18.174554	-0.050557	2.368845
265.997528	1751.178276	18.179559	-0.050557	2.364116
265.876559	1743.233442	18.184563	-0.050530	2.359366
265.967540	1735.294581	18.189568	-0.050542	2.354627
266.044767	1727.273265	18.194573	-0.050551	2.349829
265.892734	1719.326590	18.199578	-0.050517	2.345046
265.809933	1711.405237	18.204583	-0.050497	2.340275
265.889798	1703.431165	18.209587	-0.050506	2.335476
265.900867	1695.456955	18.214592	-0.050503	2.330661
265.563679	1687.550746	18.219597	-0.050435	2.325848
265.400214	1679.606572	18.224602	-0.050400	2.321017
265.573580	1671.662809	18.229607	-0.050427	2.316204
265.535146	1663.662737	18.234611	-0.050415	2.311328
265.448293	1655.723748	18.239616	-0.050393	2.306476
265.421241	1647.772659	18.244621	-0.050383	2.301611
265.279028	1639.834608	18.249626	-0.050351	2.296734
265.271011	1631.879308	18.254631	-0.050345	2.291848
265.466751	1623.875415	18.259635	-0.050376	2.286938
265.169026	1615.981888	18.264640	-0.050316	2.282044
265.044482	1608.062904	18.269645	-0.050287	2.277139
265.210965	1600.027428	18.274650	-0.050313	2.272175
265.216878	1592.044175	18.279655	-0.050309	2.267219
264.979324	1584.122393	18.284659	-0.050260	2.262270
265.020005	1576.175962	18.289664	-0.050262	2.257319
265.158431	1568.214622	18.294669	-0.050283	2.252355
264.976932	1560.258253	18.299674	-0.050244	2.247356
264.897171	1552.351717	18.304679	-0.050224	2.242386
264.899879	1544.400922	18.309683	-0.050219	2.237385
264.892278	1536.461417	18.314688	-0.050212	2.232378
264.717927	1528.521114	18.319693	-0.050175	2.227345
264.547907	1520.578563	18.324698	-0.050138	2.222299
264.664332	1512.645874	18.329703	-0.050155	2.217274
264.378551	1504.707967	18.334707	-0.050096	2.212198
264.475903	1496.730376	18.339712	-0.050109	2.207119
264.590744	1488.778598	18.344717	-0.050125	2.202047
264.431263	1480.871355	18.349722	-0.050091	2.196967
264.430145	1472.913253	18.354727	-0.050085	2.191856
264.230380	1464.943675	18.359731	-0.050043	2.186709
264.245687	1457.008667	18.364736	-0.050041	2.181590
263.989326	1449.108627	18.369741	-0.049988	2.176458
264.141447	1441.111851	18.374746	-0.050011	2.171288
264.218898	1433.168855	18.379751	-0.050020	2.166134
264.064176	1425.249288	18.384755	-0.049986	2.160962
263.793261	1417.353178	18.389760	-0.049931	2.155781
263.984123	1409.350691	18.394765	-0.049961	2.150562
264.036895	1401.392696	18.399770	-0.049966	2.145346
263.806033	1393.505302	18.404775	-0.049918	2.140137
263.944508	1385.537451	18.409779	-0.049938	2.134897
263.868454	1377.597211	18.414784	-0.049919	2.129642
263.645201	1369.698956	18.419789	-0.049872	2.124388
263.609497	1361.764734	18.424794	-0.049860	2.119115
263.784282	1353.797197	18.429799	-0.049888	2.113827
263.740850	1345.787770	18.434803	-0.049874	2.108477
263.682288	1337.872395	18.439808	-0.049858	2.103174
263.597276	1329.968752	18.444813	-0.049838	2.097863
263.693298	1322.004446	18.449818	-0.049850	2.092516
263.524694	1314.099055	18.454823	-0.049814	2.087169
263.327149	1306.191025	18.459827	-0.049772	2.081803
263.282182	1298.283601	18.464832	-0.049758	2.076439
263.259000	1290.327147	18.469837	-0.049749	2.071030
263.157251	1282.377545	18.474842	-0.049725	2.065603
263.303893	1274.434267	18.479847	-0.049747	2.060192
263.194776	1266.531398	18.484851	-0.049721	2.054768
263.088935	1258.598356	18.489856	-0.049697	2.049309
263.291085	1250.649471	18.494861	-0.049729	2.043856
263.010065	1242.765958	18.499866	-0.049672	2.038385
262.751872	1234.872977	18.504871	-0.049618	2.032894
262.968498	1226.859922	18.509875	-0.049654	2.027354
262.912493	1218.947304	18.514880	-0.049638	2.021840
262.709148	1211.064870	18.519885	-0.049595	2.016318
262.567434	1203.118882	18.524890	-0.049564	2.010742
262.714293	1195.158513	18.529895	-0.049586	2.005170
262.707355	1187.246472	18.534899	-0.049579	1.999601
262.536798	1179.360199	18.539904	-0.049542	1.994017
262.677808	1171.386605	18.544909	-0.049564	1.988389
262.698645	1163.458602	18.549914	-0.049562	1.982764
262.712550	1155.557370	18.554919	-0.049560	1.977141
262.543987	1147.640069	18.559923	-0.049523	1.971472
262.610666	1139.705715	18.564928	-0.049530	1.965799
262.350727	1131.832401	18.569933	-0.049477	1.960119
262.266594	1123.924805	18.574938	-0.049456	1.954416
262.248084	1115.958394	18.579943	-0.049448	1.948661
262.222948	1108.028763	18.584947	-0.049438	1.942915
262.068395	1100.143112	18.589952	-0.049404	1.937170
262.207082	1092.197228	18.594957	-0.049425	1.931395
261.927530	1084.298546	18.599962	-0.049367	1.925592
261.834398	1076.402119	18.604967	-0.049345	1.919794
261.853250	1068.479599	18.609971	-0.049343	1.913971
261.871153	1060.536477	18.614976	-0.049341	1.908116
261.741155	1052.656531	18.619981	-0.049312	1.902272
261.545864	1044.770871	18.624986	-0.049271	1.896399
261.742840	1036.817945	18.629991	-0.049302	1.890501
261.708191	1028.911706	18.634995	-0.049291	1.884594
261.680097	1021.026338	18.640000	-0.049280	1.878685
261.369350	1013.155553	18.645005	-0.049217	1.872736
261.720659	1005.158085	18.650010	-0.049278	1.866748
261.484866	997.302255	18.655015	-0.049229	1.860780
261.367939	989.400396	18.660019	-0.049202	1.854772
261.317667	981.489010	18.665024	-0.049187	1.848745
261.315907	973.587211	18.670029	-0.049182	1.842711
261.350258	965.682721	18.675034	-0.049183	1.836659
261.297726	957.788379	18.680039	-0.049168	1.830585
261.198595	949.869424	18.685043	-0.049145	1.824466
261.209799	941.998739	18.690048	-0.049142	1.818378
261.295122	934.089732	18.695053	-0.049152	1.812247
261.220837	926.182826	18.700058	-0.049133	1.806079
261.028518	918.331191	18.705063	-0.049092	1.799918
261.046792	910.424274	18.710067	-0.049091	1.793718
260.985929	902.477522	18.715072	-0.049074	1.787456
260.902958	894.612172	18.720077	-0.049054	1.781233
260.661431	886.747686	18.725082	-0.049004	1.774969
260.795963	878.828882	18.730087	-0.049024	1.768687
260.826234	870.929699	18.735091	-0.049024	1.762385
260.846872	863.058448	18.740096	-0.049023	1.756081
260.591815	855.197430	18.745101	-0.048970	1.749729
260.392712	847.323187	18.750106	-0.048928	1.743349
260.492913	839.444677	18.755111	-0.048942	1.736981
260.432414	831.543644	18.760115	-0.048925	1.730550
260.256066	823.694761	18.765120	-0.048887	1.724123
260.189352	815.832913	18.770125	-0.048870	1.717676
260.059944	807.933898	18.775130	-0.048841	1.711165
260.144675	800.036743	18.780135	-0.048851	1.704659
260.002400	792.183791	18.785139	-0.048820	1.698135
259.917539	784.304632	18.790144	-0.048799	1.691571
260.177699	776.383590	18.795149	-0.048842	1.684993
260.202156	768.521199	18.800154	-0.048841	1.678406
260.056770	760.673931	18.805159	-0.048809	1.671784
259.757619	752.828587	18.810163	-0.048749	1.665117
259.695362	744.980748	18.815168	-0.048732	1.658452
259.810568	737.089020	18.820173	-0.048748	1.651747
259.672644	729.227944	18.825178	-0.048717	1.645006
259.590795	721.416350	18.830183	-0.048697	1.638288
259.542947	713.501110	18.835187	-0.048683	1.631458
259.453289	705.615071	18.840192	-0.048661	1.624618
259.194805	697.805061	18.845197	-0.048608	1.617792
259.257446	689.924298	18.850202	-0.048615	1.610920
259.418374	682.053616	18.855207	-0.048639	1.604041
259.213533	674.239130	18.860211	-0.048596	1.597130
259.311276	666.359402	18.865216	-0.048609	1.590175
259.380037	658.503908	18.870221	-0.048617	1.583207
259.071319	650.704953	18.875226	-0.048555	1.576204
259.051752	642.860708	18.880231	-0.048546	1.569170
258.952934	635.031858	18.885235	-0.048522	1.562108
258.954277	627.201746	18.890240	-0.048518	1.555026
258.983907	619.328752	18.895245	-0.048518	1.547878
258.845864	611.501627	18.900250	-0.048487	1.540714
258.798180	603.681874	18.905255	-0.048473	1.533536
258.579247	595.859262	18.910259	-0.048427	1.526296
258.475515	588.057201	18.915264	-0.048403	1.519058
258.538729	580.214596	18.920269	-0.048410	1.511773
258.366870	572.400656	18.925274	-0.048373	1.504443
258.393098	564.586587	18.930279	-0.048372	1.497108
258.338035	556.756669	18.935283	-0.048357	1.489709
258.340891	548.943334	18.940288	-0.048353	1.482298
258.119975	541.170851	18.945293	-0.048306	1.474854
258.045376	533.301162	18.950298	-0.048287	1.467301
258.403658	525.444849	18.955303	-0.048349	1.459791
258.320956	517.659924	18.960307	-0.048329	1.452242
258.090957	509.892690	18.965312	-0.048281	1.444646
258.113533	502.111170	18.970317	-0.048280	1.437037
257.833312	494.329037	18.975322	-0.048223	1.429337
257.775029	486.550839	18.980327	-0.048207	1.421636
257.675832	478.770312	18.985331	-0.048183	1.413884
257.761272	470.955183	18.990336	-0.048194	1.406085
257.623421	463.215235	18.995341	-0.048163	1.398281
257.355637	455.442494	19.000346	-0.048109	1.390378
257.663804	447.615582	19.005351	-0.048161	1.382473
257.448710	439.871220	19.010355	-0.048116	1.374517
257.148472	432.134274	19.015360	-0.048055	1.366508
257.202241	424.370708	19.020365	-0.048060	1.358485
257.122120	416.596629	19.025370	-0.048040	1.350380
257.057876	408.844984	19.030375	-0.048023	1.342252
256.971722	401.110436	19.035379	-0.048002	1.334089
257.164651	393.310839	19.040384	-0.048033	1.325857
257.063456	385.607323	19.045389	-0.048009	1.317623
256.905695	377.769990	19.050394	-0.047974	1.309183
257.004271	369.996660	19.055399	-0.047988	1.300804
256.795322	362.308227	19.060403	-0.047944	1.292407
256.645482	354.603075	19.065408	-0.047911	1.283947
256.620930	346.903342	19.070413	-0.047901	1.275461
256.609153	339.168877	19.075418	-0.047894	1.266882
256.550927	331.486754	19.080423	-0.047878	1.258294
256.241855	323.818592	19.085427	-0.047816	1.249614
256.230146	316.117095	19.090432	-0.047809	1.240894
256.207305	308.429902	19.095437	-0.047799	1.232125
256.073344	300.731459	19.100442	-0.047770	1.223259
256.121879	293.048691	19.105447	-0.047774	1.214383
255.962947	285.381200	19.110451	-0.047739	1.205418
255.770834	277.747826	19.115456	-0.047698	1.196419
255.920347	270.047230	19.120461	-0.047721	1.187341
255.992788	262.375270	19.125466	-0.047730	1.178212
255.758565	254.767086	19.130471	-0.047681	1.169025
255.656571	247.134614	19.135475	-0.047657	1.159763
255.678259	239.472059	19.140480	-0.047656	1.150416
255.494845	231.853497	19.145485	-0.047617	1.141003
255.310526	224.253600	19.150490	-0.047578	1.131535
255.167075	216.661900	19.155495	-0.047546	1.122005
255.089034	209.057099	19.160499	-0.047527	1.112392
255.278908	201.419159	19.165504	-0.047557	1.102712
255.145094	193.858551	19.170509	-0.047527	1.092973
255.128131	186.273518	19.175514	-0.047519	1.083142
254.868853	178.757537	19.180519	-0.047466	1.073256
254.680083	171.201961	19.185523	-0.047426	1.063242
254.748860	163.633919	19.190528	-0.047434	1.053175
254.713698	156.098687	19.195533	-0.047423	1.043032
254.619024	148.582851	19.200538	-0.047400	1.032801
254.849516	141.024588	19.205543	-0.047438	1.022487
254.623298	133.561595	19.210547	-0.047391	1.012090
254.499610	126.086946	19.215552	-0.047363	1.001593
254.570061	118.587130	19.220557	-0.047372	0.990998
254.407950	111.116869	19.225562	-0.047337	0.980273
254.231387	103.696335	19.230567	-0.047299	0.969497
254.089961	96.274611	19.235571	-0.047268	0.958608
253.958115	88.862668	19.240576	-0.047238	0.947610
253.965552	81.454493	19.245581	-0.047235	0.936525
253.740953	74.083082	19.250586	-0.047188	0.925302
253.697763	66.723250	19.255591	-0.047176	0.914008
253.410447	59.620617	19.260595	-0.047117	0.902907