Mon Apr 19 08:44:55 2021

Number of Points = 3621
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
3.678593	0.176704	0.000000	0.000177	0.309253

3.371982	0.269577	0.005005	0.000234	0.309427
3.967371	0.185423	0.010010	0.000123	0.309539
4.011049	0.175792	0.015014	0.000115	0.309531
3.860152	0.203964	0.020019	0.000143	0.309535
3.720912	0.230494	0.025024	0.000169	0.309540
3.952089	0.188084	0.030029	0.000126	0.309538
3.827744	0.210559	0.035034	0.000149	0.309538
4.250031	0.128784	0.040038	0.000070	0.309514
4.621715	0.045565	0.045043	0.000001	0.309440
4.598136	0.004115	0.050048	0.000006	0.309226
4.170274	0.083446	0.055053	0.000085	0.309234
4.461202	0.032140	0.060058	0.000031	0.309241
4.429578	0.036038	0.065062	0.000037	0.309232
4.185992	0.080712	0.070067	0.000082	0.309234
4.324053	0.055570	0.075072	0.000057	0.309234
4.369627	0.046927	0.080077	0.000048	0.309232
4.285504	0.063605	0.085082	0.000064	0.309238
4.218511	0.073466	0.090086	0.000076	0.309227
4.419560	0.014248	0.095091	0.000039	0.309121
4.262586	-0.004768	0.100096	0.000068	0.308898
4.163443	0.012354	0.105101	0.000087	0.308894
4.361495	-0.021647	0.110106	0.000050	0.308903
4.707417	-0.089017	0.115110	-0.000014	0.308882
4.352626	-0.022030	0.120115	0.000052	0.308894
4.002644	0.022120	0.125120	0.000117	0.308803
4.197279	-0.059179	0.130125	0.000081	0.308587
4.166573	-0.053320	0.135130	0.000086	0.308588
3.743398	0.022814	0.140134	0.000165	0.308585
4.240820	-0.067471	0.145139	0.000073	0.308585
3.907646	-0.016482	0.150144	0.000135	0.308540
2.977184	0.097833	0.155149	0.000308	0.308283
3.431318	0.015370	0.160154	0.000223	0.308283
3.733252	-0.042403	0.165158	0.000167	0.308270
3.741314	-0.042803	0.170163	0.000166	0.308275
3.381448	0.020342	0.175168	0.000233	0.308264
3.686530	-0.093015	0.180173	0.000176	0.307992
4.165977	-0.182578	0.185178	0.000087	0.307980
3.541296	-0.068341	0.190182	0.000203	0.307984
3.983574	-0.157912	0.195187	0.000121	0.307940
3.936422	-0.212310	0.200192	0.000130	0.307644
3.475722	-0.129568	0.205197	0.000215	0.307640
3.742101	-0.177167	0.210202	0.000166	0.307643
3.931490	-0.254509	0.215206	0.000131	0.307441
3.841098	-0.263976	0.220211	0.000148	0.307319
3.291031	-0.161389	0.225216	0.000250	0.307331
3.782164	-0.273907	0.230221	0.000159	0.307222
2.983981	-0.169758	0.235226	0.000307	0.307029
3.062507	-0.188041	0.240230	0.000293	0.307010
3.211060	-0.213199	0.245235	0.000265	0.307019
3.375349	-0.303140	0.250240	0.000234	0.306735
3.430675	-0.319149	0.255245	0.000224	0.306707
3.592348	-0.351995	0.260250	0.000194	0.306691
3.968635	-0.491004	0.265254	0.000124	0.306357
3.616720	-0.426023	0.270259	0.000190	0.306362
3.363858	-0.407190	0.275264	0.000237	0.306234
3.655148	-0.498440	0.280269	0.000183	0.306052
3.766248	-0.517285	0.285274	0.000162	0.306059
3.253173	-0.487839	0.290278	0.000257	0.305757
2.827181	-0.409489	0.295283	0.000337	0.305761
3.388432	-0.532634	0.300288	0.000232	0.305661
2.876983	-0.475349	0.305293	0.000328	0.305492
2.862564	-0.472844	0.310298	0.000330	0.305491
2.994950	-0.557373	0.315302	0.000306	0.305205
2.458509	-0.468453	0.320307	0.000406	0.305164
2.465846	-0.490075	0.325312	0.000404	0.305068
2.608225	-0.564637	0.330317	0.000378	0.304837
2.774454	-0.593268	0.335322	0.000347	0.304844
2.546158	-0.616642	0.340326	0.000389	0.304536
2.230678	-0.563085	0.345331	0.000448	0.304518
2.395656	-0.623300	0.350336	0.000417	0.304374
2.332947	-0.643400	0.355341	0.000429	0.304224
2.454715	-0.680667	0.360346	0.000407	0.304152
2.359580	-0.719719	0.365350	0.000424	0.303884
2.552209	-0.759295	0.370355	0.000389	0.303862
2.232393	-0.761542	0.375360	0.000448	0.303574
2.653624	-0.840698	0.380365	0.000370	0.303562
2.553506	-0.885778	0.385370	0.000388	0.303260
2.530748	-0.888532	0.390374	0.000393	0.303227
2.346822	-0.911130	0.395379	0.000427	0.302959
2.475691	-0.935863	0.400384	0.000403	0.302953
1.768084	-0.875412	0.405389	0.000535	0.302627
1.714076	-0.864442	0.410394	0.000545	0.302633
1.693093	-0.923368	0.415398	0.000549	0.302333
1.920730	-0.968481	0.420403	0.000506	0.302315
1.936591	-1.035829	0.425408	0.000504	0.302006
1.675485	-0.993062	0.430413	0.000552	0.301983
1.888065	-1.090860	0.435418	0.000513	0.301699
1.556314	-1.040278	0.440422	0.000574	0.301653
1.304960	-1.053494	0.445427	0.000621	0.301370
1.543048	-1.111084	0.450432	0.000577	0.301301
1.270091	-1.112568	0.455437	0.000628	0.301056
1.112599	-1.103471	0.460442	0.000657	0.300962
0.806906	-1.093135	0.465446	0.000714	0.300744
1.254036	-1.195558	0.470451	0.000631	0.300642
1.086787	-1.196202	0.475456	0.000662	0.300493
1.040536	-1.229013	0.480461	0.000671	0.300294
1.104911	-1.266634	0.485466	0.000659	0.300169
0.891392	-1.284910	0.490470	0.000699	0.299894
1.016036	-1.322433	0.495475	0.000675	0.299822
0.941789	-1.371280	0.500480	0.000689	0.299521
1.165991	-1.436081	0.505485	0.000648	0.299404
0.391532	-1.328692	0.510490	0.000792	0.299243
0.260987	-1.348244	0.515494	0.000816	0.299033
0.303325	-1.382732	0.520499	0.000808	0.298904
0.073108	-1.394733	0.525504	0.000851	0.298643
0.220684	-1.441938	0.530509	0.000824	0.298544
0.591444	-1.568081	0.535514	0.000755	0.298259
0.228989	-1.528757	0.540518	0.000822	0.298130
0.111506	-1.541486	0.545523	0.000844	0.297964
0.055548	-1.583510	0.550528	0.000855	0.297711
0.085463	-1.614578	0.555533	0.000849	0.297586
0.001491	-1.654527	0.560538	0.000865	0.297317
-0.044975	-1.681816	0.565542	0.000874	0.297143
0.052964	-1.731935	0.570547	0.000855	0.296986
-0.013651	-1.775619	0.575552	0.000868	0.296714
-0.258099	-1.761402	0.580557	0.000913	0.296566
-0.355418	-1.784793	0.585562	0.000932	0.296366
-0.552051	-1.799702	0.590566	0.000968	0.296118
-0.770568	-1.786129	0.595571	0.001009	0.295990
-0.935969	-1.805700	0.600576	0.001040	0.295747
-0.887673	-1.847173	0.605581	0.001031	0.295587
-1.232020	-1.801888	0.610586	0.001095	0.295502
-1.525605	-1.815414	0.615590	0.001150	0.295175
-1.398732	-1.864553	0.620595	0.001126	0.295047
-1.764332	-1.838202	0.625600	0.001194	0.294850
-2.118484	-1.824483	0.630605	0.001260	0.294601
-2.156140	-1.835527	0.635610	0.001267	0.294513
-1.730982	-1.974025	0.640614	0.001188	0.294212
-1.739305	-2.006658	0.645619	0.001190	0.294044
-1.958731	-2.000659	0.650624	0.001230	0.293877
-1.857222	-2.077062	0.655629	0.001212	0.293591
-2.005067	-2.078886	0.660634	0.001239	0.293450
-2.201847	-2.085629	0.665638	0.001276	0.293240
-2.217736	-2.130924	0.670643	0.001279	0.293002
-2.485556	-2.110396	0.675648	0.001329	0.292863
-2.480878	-2.163612	0.680653	0.001328	0.292604
-2.502089	-2.204349	0.685658	0.001332	0.292383
-2.879693	-2.165034	0.690662	0.001402	0.292238
-3.285904	-2.143090	0.695667	0.001478	0.291981
-3.493054	-2.138172	0.700672	0.001516	0.291818
-3.480904	-2.166512	0.705677	0.001514	0.291688
-3.836801	-2.165445	0.710682	0.001581	0.291373
-3.958335	-2.167606	0.715686	0.001603	0.291252
-3.650985	-2.264620	0.720691	0.001546	0.291047
-3.904554	-2.266440	0.725696	0.001593	0.290809
-4.132028	-2.251761	0.730701	0.001636	0.290676
-4.598790	-2.201727	0.735706	0.001723	0.290503
-4.268690	-2.303436	0.740710	0.001661	0.290295
-4.868794	-2.223827	0.745715	0.001773	0.290147
-5.139861	-2.231939	0.750720	0.001823	0.289861
-5.154047	-2.252850	0.755725	0.001826	0.289744
-4.947010	-2.340651	0.760730	0.001788	0.289493
-5.329099	-2.305720	0.765734	0.001859	0.289320
-5.095237	-2.372264	0.770739	0.001815	0.289200
-5.327137	-2.395390	0.775744	0.001858	0.288873
-5.520440	-2.386929	0.780749	0.001894	0.288739
-5.954492	-2.342903	0.785754	0.001975	0.288564
-6.110552	-2.361098	0.790758	0.002004	0.288330
-6.625355	-2.285120	0.795763	0.002100	0.288242
-6.510697	-2.364176	0.800768	0.002079	0.287949
-6.455295	-2.398098	0.805773	0.002069	0.287829
-7.095981	-2.323820	0.810778	0.002188	0.287617
-7.253260	-2.330673	0.815782	0.002217	0.287438
-7.363408	-2.339460	0.820787	0.002238	0.287293
-7.147979	-2.429481	0.825792	0.002198	0.287037
-7.581549	-2.367987	0.830797	0.002278	0.286949
-7.762710	-2.387335	0.835802	0.002312	0.286685
-8.223544	-2.316929	0.840806	0.002398	0.286618
-8.412568	-2.335114	0.845811	0.002433	0.286352
-8.347323	-2.368635	0.850816	0.002421	0.286242
-8.180036	-2.441350	0.855821	0.002390	0.286028
-8.745147	-2.370552	0.860826	0.002495	0.285867
-9.037597	-2.345332	0.865830	0.002550	0.285725
-9.072078	-2.372498	0.870835	0.002556	0.285555
-9.431112	-2.320891	0.875840	0.002623	0.285486
-9.471515	-2.368439	0.880845	0.002631	0.285208
-9.506722	-2.375508	0.885850	0.002637	0.285139
-9.587321	-2.416979	0.890854	0.002652	0.284854
-10.002441	-2.349868	0.895859	0.002729	0.284811
-10.133178	-2.385542	0.900864	0.002754	0.284509
-10.242194	-2.371384	0.905869	0.002774	0.284480
-10.250784	-2.425158	0.910874	0.002776	0.284198
-10.632355	-2.358375	0.915878	0.002847	0.284185
-10.907091	-2.371800	0.920883	0.002898	0.283862
-10.868112	-2.382225	0.925888	0.002891	0.283845
-11.496716	-2.326067	0.930893	0.003008	0.283548
-11.272736	-2.365083	0.935898	0.002966	0.283557
-11.444006	-2.397643	0.940902	0.002998	0.283231
-11.782904	-2.337367	0.945907	0.003061	0.283224
-11.958823	-2.357271	0.950912	0.003094	0.282959
-11.984697	-2.358484	0.955917	0.003099	0.282928
-12.140519	-2.382966	0.960922	0.003128	0.282658
-12.516134	-2.326583	0.965926	0.003198	0.282597
-12.287051	-2.412311	0.970931	0.003155	0.282371
-12.564176	-2.379483	0.975936	0.003207	0.282281
-12.936726	-2.352772	0.980941	0.003276	0.282070
-13.081100	-2.347037	0.985946	0.003303	0.281965
-13.233377	-2.345663	0.990950	0.003332	0.281830
-13.379245	-2.352948	0.995955	0.003359	0.281656
-13.722756	-2.301288	1.000960	0.003423	0.281600
-14.374554	-2.231765	1.005965	0.003544	0.281348
-14.164455	-2.269968	1.010970	0.003505	0.281348
-14.261033	-2.304490	1.015974	0.003523	0.281080
-14.681619	-2.236213	1.020979	0.003601	0.281038
-14.615204	-2.276681	1.025984	0.003589	0.280891
-14.767335	-2.285180	1.030989	0.003617	0.280705
-14.647086	-2.311541	1.035994	0.003595	0.280681
-15.103122	-2.266524	1.040998	0.003680	0.280486
-15.026353	-2.282257	1.046003	0.003666	0.280476
-14.955887	-2.345948	1.051008	0.003652	0.280214
-15.428442	-2.274399	1.056013	0.003740	0.280139
-15.499013	-2.288112	1.061018	0.003754	0.280002
-15.824510	-2.263576	1.066022	0.003814	0.279823
-16.125477	-2.207660	1.071027	0.003870	0.279829
-16.304476	-2.236369	1.076032	0.003904	0.279512
-16.465386	-2.210717	1.081037	0.003934	0.279493
-16.399469	-2.247134	1.086042	0.003921	0.279366
-16.156733	-2.321070	1.091046	0.003876	0.279211
-16.520472	-2.261276	1.096051	0.003944	0.279178
-16.564036	-2.313025	1.101056	0.003952	0.278869
-17.430175	-2.152049	1.106061	0.004113	0.278887
-17.533913	-2.163661	1.111066	0.004133	0.278728
-17.946161	-2.116122	1.116070	0.004209	0.278586
-17.622558	-2.176796	1.121075	0.004149	0.278576
-17.423812	-2.264681	1.126080	0.004112	0.278307
-18.073222	-2.156789	1.131085	0.004233	0.278254
-17.583351	-2.264491	1.136090	0.004142	0.278157
-17.611192	-2.298819	1.141094	0.004147	0.277952
-18.017147	-2.224627	1.146099	0.004223	0.277954
-18.349286	-2.216690	1.151104	0.004285	0.277680
-18.597182	-2.183147	1.156109	0.004331	0.277620
-18.366625	-2.239321	1.161114	0.004288	0.277545
-18.427647	-2.275348	1.166118	0.004299	0.277299
-18.366956	-2.287768	1.171123	0.004288	0.277292
-18.530423	-2.306046	1.176128	0.004319	0.277041
-19.012439	-2.231880	1.181133	0.004408	0.276971
-19.141695	-2.224606	1.186138	0.004432	0.276886
-19.195152	-2.251481	1.191142	0.004442	0.276694
-19.511338	-2.194197	1.196147	0.004501	0.276693
-19.646257	-2.214002	1.201152	0.004526	0.276461
-19.891375	-2.190142	1.206157	0.004572	0.276352
-19.329151	-2.303195	1.211162	0.004467	0.276295
-19.822246	-2.261545	1.216166	0.004559	0.276044
-19.838535	-2.259849	1.221171	0.004562	0.276037
-19.906773	-2.285432	1.226176	0.004575	0.275837
-20.616569	-2.175907	1.231181	0.004707	0.275735
-20.237250	-2.249303	1.236186	0.004637	0.275711
-20.376724	-2.266279	1.241190	0.004663	0.275489
-20.431161	-2.258137	1.246195	0.004673	0.275479
-20.418037	-2.299362	1.251200	0.004670	0.275275
-20.621006	-2.289133	1.256205	0.004708	0.275135
-20.920209	-2.241315	1.261210	0.004764	0.275100
-21.316463	-2.221909	1.266214	0.004838	0.274822
-21.360948	-2.214746	1.271219	0.004846	0.274817
-21.129224	-2.289872	1.276224	0.004803	0.274644
-21.520031	-2.247248	1.281229	0.004876	0.274493
-21.749381	-2.205403	1.286234	0.004918	0.274494
-22.042453	-2.204520	1.291238	0.004973	0.274217
-21.867853	-2.237168	1.296243	0.004940	0.274212
-21.963985	-2.245691	1.301248	0.004958	0.274075
-22.341057	-2.216523	1.306253	0.005029	0.273867
-22.342722	-2.214693	1.311258	0.005029	0.273875
-22.352608	-2.262717	1.316262	0.005031	0.273611
-22.434720	-2.259584	1.321267	0.005046	0.273548
-22.114525	-2.336446	1.326272	0.004987	0.273450
-22.813596	-2.250163	1.331277	0.005117	0.273233
-23.006650	-2.213732	1.336282	0.005153	0.273240
-23.090116	-2.240646	1.341286	0.005168	0.273017
-23.098275	-2.252982	1.346291	0.005170	0.272943
-23.271565	-2.234366	1.351296	0.005202	0.272875
-23.427702	-2.256722	1.356301	0.005231	0.272605
-23.321639	-2.275483	1.361306	0.005211	0.272608
-23.616079	-2.261709	1.366310	0.005266	0.272397
-24.101433	-2.191982	1.371315	0.005357	0.272298
-23.518325	-2.305873	1.376320	0.005248	0.272256
-24.121282	-2.249673	1.381325	0.005360	0.271972
-24.591476	-2.162203	1.386330	0.005448	0.271982
-24.681003	-2.169778	1.391334	0.005465	0.271855
-24.532711	-2.229118	1.396339	0.005437	0.271682
-24.564260	-2.222019	1.401344	0.005443	0.271689
-25.037876	-2.189864	1.406349	0.005531	0.271401
-24.722647	-2.256910	1.411354	0.005473	0.271349
-24.709060	-2.273302	1.416358	0.005470	0.271275
-25.414797	-2.187568	1.421363	0.005601	0.271047
-25.494612	-2.170689	1.426368	0.005616	0.271060
-25.550805	-2.194230	1.431373	0.005627	0.270879
-26.142694	-2.111292	1.436378	0.005737	0.270747
-25.995033	-2.137923	1.441382	0.005710	0.270748
-25.779903	-2.215934	1.446387	0.005670	0.270540
-25.980395	-2.189349	1.451392	0.005707	0.270487
-26.526385	-2.094979	1.456397	0.005809	0.270461
-26.312182	-2.194249	1.461402	0.005769	0.270137
-26.348418	-2.188019	1.466406	0.005775	0.270135
-26.555403	-2.173790	1.471411	0.005814	0.270010
-26.519037	-2.216128	1.476416	0.005807	0.269818
-26.473334	-2.225699	1.481421	0.005799	0.269811
-26.565012	-2.257118	1.486426	0.005816	0.269553
-27.093375	-2.172711	1.491430	0.005914	0.269490
-26.940224	-2.212974	1.496435	0.005886	0.269423
-26.952780	-2.250773	1.501440	0.005888	0.269207
-27.421232	-2.165067	1.506445	0.005975	0.269210
-27.567481	-2.173949	1.511450	0.006003	0.269019
-27.592492	-2.197147	1.516454	0.006007	0.268869
-27.775104	-2.165036	1.521459	0.006041	0.268863
-28.004536	-2.172686	1.526464	0.006084	0.268597
-28.190546	-2.144740	1.531469	0.006119	0.268565
-28.068208	-2.181950	1.536474	0.006096	0.268485
-28.296242	-2.186912	1.541478	0.006138	0.268234
-28.256948	-2.193781	1.546483	0.006131	0.268235
-28.441042	-2.187240	1.551488	0.006165	0.268090
-28.851967	-2.137647	1.556493	0.006242	0.267954
-28.808901	-2.144452	1.561498	0.006234	0.267959
-28.854648	-2.190080	1.566502	0.006243	0.267667
-29.254614	-2.128028	1.571507	0.006317	0.267609
-29.156738	-2.154438	1.576512	0.006299	0.267563
-29.539274	-2.133967	1.581517	0.006370	0.267297
-29.323226	-2.174442	1.586522	0.006330	0.267290
-29.294005	-2.207641	1.591526	0.006325	0.267139
-29.745986	-2.157307	1.596531	0.006409	0.266966
-29.596177	-2.182232	1.601536	0.006381	0.266978
-30.148860	-2.129388	1.606541	0.006484	0.266720
-30.121291	-2.139563	1.611546	0.006479	0.266691
-30.250511	-2.122103	1.616550	0.006503	0.266659
-30.846633	-2.068751	1.621555	0.006614	0.266359
-31.041652	-2.030008	1.626560	0.006650	0.266377
-30.710396	-2.104671	1.631565	0.006588	0.266298
-31.326301	-2.035338	1.636570	0.006703	0.266066
-31.104163	-2.075529	1.641574	0.006662	0.266067
-30.687811	-2.177462	1.646579	0.006584	0.265924
-31.063794	-2.144903	1.651584	0.006654	0.265729
-31.605021	-2.045553	1.656589	0.006755	0.265734
-31.398326	-2.114263	1.661594	0.006717	0.265564
-31.399745	-2.130134	1.666598	0.006717	0.265476
-32.001313	-2.019709	1.671603	0.006829	0.265481
-31.808467	-2.109723	1.676608	0.006793	0.265181
-31.946983	-2.093792	1.681613	0.006819	0.265131
-31.850937	-2.122950	1.686618	0.006801	0.265067
-32.161853	-2.111918	1.691622	0.006859	0.264818
-32.104801	-2.124901	1.696627	0.006848	0.264803
-32.246110	-2.128778	1.701632	0.006875	0.264641
-32.939181	-2.031577	1.706637	0.007004	0.264483
-32.723764	-2.071436	1.711642	0.006964	0.264479
-32.436568	-2.159016	1.716646	0.006910	0.264286
-33.080440	-2.059432	1.721651	0.007030	0.264190
-32.628565	-2.145841	1.726656	0.006946	0.264166
-32.913287	-2.152359	1.731661	0.006999	0.263846
-32.968987	-2.140748	1.736666	0.007009	0.263854
-33.056128	-2.150967	1.741670	0.007026	0.263711
-33.424538	-2.114900	1.746675	0.007094	0.263541
-33.369318	-2.123123	1.751680	0.007084	0.263551
-33.663751	-2.122616	1.756685	0.007139	0.263259
-33.608854	-2.139295	1.761690	0.007129	0.263222
-33.630632	-2.148769	1.766694	0.007133	0.263148
-34.398215	-2.048879	1.771699	0.007276	0.262929
-34.057110	-2.109870	1.776704	0.007212	0.262935
-33.789575	-2.195566	1.781709	0.007162	0.262731
-34.473317	-2.095371	1.786714	0.007290	0.262597
-34.538393	-2.082960	1.791718	0.007302	0.262600
-34.570118	-2.135974	1.796723	0.007308	0.262276
-34.527783	-2.141658	1.801728	0.007300	0.262287
-34.863935	-2.104143	1.806733	0.007362	0.262156
-35.041074	-2.108706	1.811738	0.007396	0.261953
-34.738495	-2.163527	1.816742	0.007339	0.261954
-35.287663	-2.106369	1.821747	0.007441	0.261717
-35.297110	-2.113602	1.826752	0.007443	0.261668
-34.862158	-2.207817	1.831757	0.007362	0.261584
-35.252899	-2.183963	1.836762	0.007435	0.261322
-35.374961	-2.160828	1.841766	0.007458	0.261327
-35.508940	-2.179725	1.846771	0.007483	0.261087
-35.463337	-2.200021	1.851776	0.007474	0.261021
-35.799356	-2.155665	1.856781	0.007537	0.260927
-36.251171	-2.113636	1.861786	0.007621	0.260704
-35.938607	-2.169514	1.866790	0.007563	0.260710
-36.349766	-2.128024	1.871795	0.007639	0.260524
-36.489926	-2.111925	1.876800	0.007666	0.260472
-35.958212	-2.224486	1.881805	0.007567	0.260384
-36.145731	-2.238483	1.886810	0.007602	0.260116
-36.537326	-2.167145	1.891814	0.007674	0.260117
-37.039431	-2.124270	1.896819	0.007768	0.259846
-37.191032	-2.102872	1.901824	0.007796	0.259812
-36.984150	-2.157612	1.906829	0.007758	0.259716
-37.326171	-2.138793	1.911834	0.007821	0.259474
-37.103448	-2.177938	1.916838	0.007780	0.259482
-37.258735	-2.192195	1.921843	0.007809	0.259244
-37.446940	-2.167507	1.926848	0.007844	0.259191
-37.475333	-2.182726	1.931853	0.007849	0.259077
-38.083684	-2.110405	1.936858	0.007963	0.258862
-38.167213	-2.095268	1.941862	0.007978	0.258862
-38.278440	-2.118288	1.946867	0.007999	0.258619
-38.428470	-2.102339	1.951872	0.008027	0.258556
-38.495881	-2.097999	1.956877	0.008039	0.258511
-38.961259	-2.063627	1.961882	0.008126	0.258229
-38.764888	-2.098127	1.966886	0.008090	0.258236
-38.679851	-2.142610	1.971891	0.008074	0.258073
-38.777811	-2.149359	1.976896	0.008092	0.257935
-38.995884	-2.108889	1.981901	0.008133	0.257939
-38.925769	-2.182978	1.986906	0.008120	0.257594
-39.208124	-2.130095	1.991910	0.008172	0.257603
-39.589026	-2.088239	1.996915	0.008243	0.257448
-39.509336	-2.131642	2.001920	0.008228	0.257286

-39.871764	-2.118903	2.011917	0.008296	0.256986
-39.945535	-2.131032	2.021914	0.008310	0.256841
-40.167357	-2.121058	2.031910	0.008351	0.256670
-40.512630	-2.094896	2.041907	0.008415	0.256463
-40.448188	-2.128868	2.051904	0.008403	0.256337
-40.538134	-2.132535	2.061901	0.008420	0.256223
-40.678496	-2.142374	2.071898	0.008446	0.256023
-40.805637	-2.120315	2.081894	0.008470	0.256017
-41.053198	-2.097504	2.091891	0.008516	0.255891
-40.999667	-2.139196	2.101888	0.008506	0.255709
-41.497998	-2.047201	2.111885	0.008599	0.255717
-41.188271	-2.104535	2.121882	0.008541	0.255711
-41.517474	-2.043848	2.131878	0.008603	0.255715
-40.888487	-2.160655	2.141875	0.008486	0.255702
-40.904725	-2.155806	2.151872	0.008489	0.255712
-41.526032	-2.041060	2.161869	0.008604	0.255721
-41.206440	-2.100776	2.171866	0.008545	0.255712
-41.431106	-2.059650	2.181862	0.008587	0.255713
-41.259223	-2.089942	2.191859	0.008555	0.255719
-41.069690	-2.125036	2.201856	0.008520	0.255715
-41.417189	-2.060831	2.211853	0.008584	0.255720
-41.111888	-2.118357	2.221850	0.008528	0.255709
-41.427131	-2.028794	2.231846	0.008586	0.255891
-41.126627	-2.057462	2.241843	0.008530	0.256038
-40.986216	-2.083985	2.251840	0.008504	0.256032
-41.252242	-2.033895	2.261837	0.008554	0.256042
-40.778002	-2.072494	2.271834	0.008466	0.256311
-41.082247	-2.011169	2.281830	0.008522	0.256344
-40.988806	-2.022438	2.291827	0.008505	0.256377
-40.730716	-2.014095	2.301824	0.008457	0.256689
-40.820523	-1.997817	2.311821	0.008474	0.256688
-40.304005	-2.060160	2.321818	0.008378	0.256866
-40.467579	-2.012978	2.331814	0.008408	0.256964
-40.107455	-2.058548	2.341811	0.008341	0.257076
-39.727887	-2.091154	2.351808	0.008271	0.257281
-40.147695	-2.004273	2.361805	0.008349	0.257340
-40.090859	-1.965392	2.371802	0.008338	0.257617
-40.498791	-1.865169	2.381798	0.008414	0.257763
-39.472519	-2.018419	2.391795	0.008223	0.257951
-39.242912	-2.032276	2.401792	0.008180	0.258107
-39.055946	-2.045915	2.411789	0.008146	0.258221
-38.283261	-2.149373	2.421786	0.008002	0.258429
-38.585554	-2.076473	2.431782	0.008058	0.258529
-38.130880	-2.121472	2.441779	0.007974	0.258740
-38.383603	-2.055274	2.451776	0.008021	0.258853
-38.112647	-2.052546	2.461773	0.007970	0.259144
-37.932165	-2.072283	2.471770	0.007937	0.259217
-37.744533	-2.060707	2.481766	0.007902	0.259472
-37.455081	-2.088597	2.491763	0.007848	0.259610
-37.587122	-2.028750	2.501760	0.007873	0.259809
-38.093573	-1.885793	2.511757	0.007967	0.260092
-37.674688	-1.922909	2.521754	0.007889	0.260309
-38.272741	-1.773986	2.531750	0.008000	0.260532
-37.660022	-1.848591	2.541747	0.007886	0.260737
-37.195649	-1.884069	2.551744	0.007800	0.261009
-37.024257	-1.875472	2.561741	0.007768	0.261229
-36.697256	-1.899357	2.571738	0.007707	0.261426
-36.472118	-1.893399	2.581734	0.007665	0.261686
-36.319348	-1.872583	2.591731	0.007637	0.261954
-36.225853	-1.850307	2.601728	0.007619	0.262171
-35.435573	-1.957966	2.611725	0.007472	0.262370
-34.902924	-2.014285	2.621722	0.007373	0.262594
-34.639687	-2.011641	2.631718	0.007324	0.262872
-34.420577	-2.024266	2.641715	0.007284	0.263022
-34.624402	-1.949171	2.651712	0.007321	0.263231
-34.032099	-2.002733	2.661709	0.007211	0.263529
-34.387596	-1.901771	2.671706	0.007277	0.263728
-34.146821	-1.906285	2.681702	0.007233	0.263943
-33.416545	-1.991622	2.691699	0.007097	0.264204
-33.274884	-1.974467	2.701696	0.007070	0.264439
-32.568080	-2.068872	2.711693	0.006939	0.264625
-32.757955	-2.001610	2.721690	0.006974	0.264804
-32.613230	-1.969818	2.731686	0.006947	0.265122
-32.366244	-1.970849	2.741683	0.006901	0.265361
-32.391543	-1.930820	2.751680	0.006906	0.265554
-31.600571	-2.044940	2.761677	0.006759	0.265716
-31.991119	-1.916344	2.771674	0.006832	0.266029
-31.677189	-1.930304	2.781670	0.006773	0.266264
-31.384134	-1.942169	2.791667	0.006719	0.266489
-31.651337	-1.844318	2.801664	0.006768	0.266756
-30.789620	-1.961237	2.811661	0.006608	0.266972
-30.883869	-1.889827	2.821658	0.006626	0.267266
-30.293227	-1.952211	2.831654	0.006516	0.267510
-30.313647	-1.908459	2.841651	0.006520	0.267726
-29.616272	-1.992007	2.851648	0.006390	0.267960
-29.444775	-1.972335	2.861645	0.006358	0.268234
-29.375794	-1.942543	2.871642	0.006345	0.268463
-28.974377	-1.976456	2.881638	0.006270	0.268673
-28.741093	-1.978361	2.891635	0.006227	0.268891
-28.483004	-1.968308	2.901632	0.006179	0.269198
-28.499746	-1.924225	2.911629	0.006182	0.269418
-28.289433	-1.917538	2.921626	0.006143	0.269659
-27.719439	-1.980551	2.931622	0.006037	0.269877
-27.425058	-1.987381	2.941619	0.005982	0.270128
-27.312584	-1.950356	2.951616	0.005961	0.270435
-27.287603	-1.919804	2.961613	0.005957	0.270623
-26.954004	-1.941933	2.971610	0.005895	0.270829
-26.644730	-1.955899	2.981606	0.005837	0.271055
-26.438724	-1.938319	2.991603	0.005799	0.271348
-26.208827	-1.931856	3.001600	0.005756	0.271606
-25.741026	-1.976497	3.011597	0.005669	0.271821
-26.081746	-1.870242	3.021594	0.005732	0.272056
-25.540190	-1.923412	3.031590	0.005632	0.272297
-24.947208	-1.974068	3.041587	0.005521	0.272601
-24.857198	-1.947575	3.051584	0.005505	0.272828
-24.702840	-1.932535	3.061581	0.005476	0.273057
-24.690228	-1.892437	3.071578	0.005473	0.273281
-24.402593	-1.892302	3.081574	0.005420	0.273559
-23.984449	-1.915988	3.091571	0.005342	0.273836
-23.825107	-1.897168	3.101568	0.005313	0.274088
-23.989847	-1.818473	3.111565	0.005343	0.274345
-23.963873	-1.773779	3.121562	0.005338	0.274605
-23.483971	-1.809258	3.131558	0.005249	0.274878
-23.352315	-1.779679	3.141555	0.005225	0.275160
-22.770200	-1.824786	3.151552	0.005116	0.275479
-22.901918	-1.761772	3.161549	0.005141	0.275684
-22.205978	-1.841909	3.171546	0.005011	0.275927
-22.059846	-1.822446	3.181542	0.004984	0.276169
-22.091679	-1.764879	3.191539	0.004990	0.276440
-21.523729	-1.817474	3.201536	0.004884	0.276705
-21.121878	-1.838655	3.211533	0.004810	0.276976
-20.931230	-1.822991	3.221530	0.004774	0.277239
-20.944326	-1.771679	3.231526	0.004777	0.277494
-20.545750	-1.793869	3.241523	0.004702	0.277756
-20.175264	-1.809658	3.251520	0.004634	0.278024
-20.368110	-1.725689	3.261517	0.004669	0.278279
-19.626974	-1.803616	3.271514	0.004532	0.278574
-19.500083	-1.780359	3.281510	0.004508	0.278815
-19.027213	-1.817172	3.291507	0.004420	0.279070
-18.771486	-1.819652	3.301504	0.004372	0.279298
-18.851685	-1.758342	3.311501	0.004387	0.279539
-18.265137	-1.809105	3.321498	0.004278	0.279829
-17.842199	-1.836671	3.331494	0.004199	0.280083
-17.931717	-1.769467	3.341491	0.004216	0.280346
-17.832368	-1.742972	3.351488	0.004198	0.280576
-17.640596	-1.737536	3.361485	0.004162	0.280784
-17.310620	-1.745592	3.371482	0.004101	0.281051
-17.450090	-1.659782	3.381478	0.004127	0.281362
-16.933907	-1.697961	3.391475	0.004031	0.281648
-16.340615	-1.762454	3.401472	0.003920	0.281871
-16.094613	-1.761203	3.411469	0.003874	0.282107
-15.735355	-1.780715	3.421466	0.003808	0.282341
-15.437607	-1.784507	3.431462	0.003752	0.282599
-15.169641	-1.772426	3.441459	0.003702	0.282910
-14.796630	-1.797964	3.451456	0.003633	0.283126
-15.105797	-1.694315	3.461453	0.003690	0.283369
-14.472743	-1.762918	3.471450	0.003573	0.283606
-13.934138	-1.810258	3.481446	0.003472	0.283864
-13.755703	-1.788427	3.491443	0.003439	0.284140
-13.676727	-1.759048	3.501440	0.003425	0.284363
-13.234579	-1.800222	3.511437	0.003342	0.284562
-13.299377	-1.733950	3.521434	0.003354	0.284839
-12.901285	-1.749209	3.531430	0.003280	0.285129
-12.568282	-1.762070	3.541427	0.003218	0.285370
-12.355952	-1.759843	3.551424	0.003179	0.285577
-12.140054	-1.761803	3.561421	0.003139	0.285766
-12.203311	-1.691812	3.571418	0.003150	0.286062
-12.375653	-1.605145	3.581414	0.003183	0.286341
-11.753653	-1.665110	3.591411	0.003067	0.286610
-11.491763	-1.665140	3.601408	0.003018	0.286850
-11.197235	-1.672738	3.611405	0.002963	0.287081
-11.031462	-1.653163	3.621402	0.002932	0.287331
-11.141701	-1.571891	3.631398	0.002953	0.287639
-10.588858	-1.610581	3.641395	0.002850	0.287950
-10.167979	-1.642988	3.651392	0.002772	0.288172
-9.922022	-1.639279	3.661389	0.002726	0.288414
-10.225624	-1.528325	3.671386	0.002783	0.288694
-9.499807	-1.611161	3.681382	0.002648	0.288940
-9.261069	-1.599446	3.691379	0.002603	0.289216
-9.666617	-1.464404	3.701376	0.002679	0.289522
-9.090682	-1.512570	3.711373	0.002571	0.289804
-8.792482	-1.514325	3.721370	0.002516	0.290066
-8.641864	-1.485642	3.731366	0.002488	0.290345
-8.498533	-1.457522	3.741363	0.002461	0.290615
-8.292057	-1.446637	3.751360	0.002423	0.290856
-7.981216	-1.445645	3.761357	0.002365	0.291142
-7.927391	-1.398902	3.771354	0.002355	0.291422
-8.048277	-1.310934	3.781350	0.002377	0.291750
-7.519673	-1.355757	3.791347	0.002279	0.292004
-6.781897	-1.428060	3.801344	0.002142	0.292310
-6.564060	-1.412529	3.811341	0.002101	0.292582
-6.585765	-1.350185	3.821338	0.002105	0.292871
-6.580743	-1.292702	3.831334	0.002104	0.293159
-6.655214	-1.217107	3.841331	0.002118	0.293465
-6.216229	-1.236998	3.851328	0.002037	0.293760
-6.198518	-1.174565	3.861325	0.002033	0.294083
-5.616202	-1.223810	3.871322	0.001925	0.294361
-5.813294	-1.124785	3.881318	0.001962	0.294671
-5.338783	-1.147147	3.891315	0.001873	0.294985
-5.108634	-1.126465	3.901312	0.001831	0.295291
-5.135985	-1.056959	3.911309	0.001836	0.295607
-4.525691	-1.115939	3.921306	0.001722	0.295861
-4.578828	-1.041417	3.931302	0.001732	0.296178
-4.496551	-0.989180	3.941299	0.001717	0.296506
-3.979781	-1.018948	3.951296	0.001620	0.296819
-3.880311	-0.975322	3.961293	0.001602	0.297119
-3.997565	-0.886148	3.971290	0.001624	0.297449
-4.151437	-0.783546	3.981286	0.001652	0.297812
-3.757696	-0.784582	3.991283	0.001579	0.298154
-3.467214	-0.768461	4.001280	0.001525	0.298488
-3.289493	-0.730224	4.011277	0.001492	0.298830
-2.652446	-0.775856	4.021274	0.001373	0.299169
-2.741290	-0.694499	4.031270	0.001390	0.299484
-2.375125	-0.685130	4.041267	0.001322	0.299851
-2.005301	-0.682453	4.051264	0.001253	0.300188
-2.050796	-0.603128	4.061261	0.001261	0.300530
-1.900671	-0.569496	4.071258	0.001234	0.300823
-1.879968	-0.499163	4.081254	0.001230	0.301179
-1.447398	-0.503794	4.091251	0.001149	0.301534
-1.624148	-0.397909	4.101248	0.001182	0.301887
-1.558111	-0.333605	4.111245	0.001170	0.302253
-1.306917	-0.293749	4.121242	0.001123	0.302662
-0.917981	-0.285079	4.131238	0.001051	0.303040
-0.564314	-0.277236	4.141235	0.000985	0.303384
-0.280813	-0.252943	4.151232	0.000932	0.303746
-0.364144	-0.157773	4.161229	0.000948	0.304126
-0.667987	-0.017347	4.171226	0.001004	0.304531
-0.597646	0.060402	4.181222	0.000991	0.304961
-0.204131	0.074199	4.191219	0.000918	0.305365
-0.226590	0.157756	4.201216	0.000922	0.305741
0.000000	0.207891	4.211213	0.000880	0.306173

0.341685	0.409598	4.216218	0.000816	0.307417
1.515394	0.754211	4.221222	0.000597	0.310032
2.692555	1.390857	4.226227	0.000378	0.313976
4.312901	2.238486	4.231232	0.000075	0.319195
6.944347	3.201785	4.236237	-0.000415	0.325662
10.293685	4.352459	4.241242	-0.001040	0.333384
14.043920	5.749287	4.246246	-0.001739	0.342280
18.125331	7.429492	4.251251	-0.002500	0.352362
22.461809	9.392480	4.256256	-0.003308	0.363473
26.270146	11.805151	4.261261	-0.004019	0.375617
29.550264	14.680353	4.266266	-0.004632	0.388746
36.376712	17.277033	4.271270	-0.005904	0.402751
45.681537	19.852810	4.276275	-0.007639	0.417764
48.975818	23.923039	4.281280	-0.008255	0.433608
51.409973	28.514133	4.286285	-0.008711	0.450066
54.092018	33.445471	4.291290	-0.009213	0.467133
57.192299	38.670867	4.296294	-0.009794	0.484700
61.182467	44.125927	4.301299	-0.010541	0.502771
68.141702	49.437617	4.306304	-0.011840	0.521299
79.011444	54.464118	4.311309	-0.013867	0.540305
84.858487	60.820223	4.316314	-0.014960	0.559757
88.633403	67.897757	4.321318	-0.015667	0.579419
91.904565	75.397723	4.326323	-0.016281	0.599234
94.630291	83.294617	4.331328	-0.016794	0.619108
97.995107	91.346390	4.336333	-0.017426	0.638971
102.186757	99.528528	4.341338	-0.018212	0.658841
106.507266	107.934653	4.346342	-0.019022	0.678650
111.841141	116.396628	4.351347	-0.020020	0.698383
115.577326	125.355708	4.356352	-0.020722	0.717996
119.999931	134.367753	4.361357	-0.021551	0.737426
124.745642	143.506588	4.366362	-0.022441	0.756705
128.145093	153.013894	4.371366	-0.023080	0.775741
131.034148	162.716033	4.376371	-0.023624	0.794507
135.074712	172.286955	4.381376	-0.024383	0.812966
141.215475	181.589269	4.386381	-0.025532	0.831190
148.755854	190.735572	4.391386	-0.026942	0.849172
155.860727	200.072075	4.396390	-0.028271	0.866964
160.111527	209.955088	4.401395	-0.029069	0.884464
164.809093	219.780364	4.406400	-0.029950	0.901653
169.929738	229.537939	4.411405	-0.030910	0.918528
175.404403	239.227187	4.416410	-0.031935	0.935085
179.195784	249.205406	4.421414	-0.032648	0.951340
182.902530	259.146316	4.426419	-0.033345	0.967242
186.702755	269.037791	4.431424	-0.034059	0.982836
190.780821	278.822349	4.436429	-0.034824	0.998098
194.743380	288.554057	4.441434	-0.035568	1.013024
198.130510	298.321699	4.446438	-0.036205	1.027641
201.803010	307.968522	4.451443	-0.036895	1.041952
205.694748	317.533626	4.456448	-0.037626	1.056007
208.466855	327.212792	4.461453	-0.038149	1.069767
211.989012	336.681268	4.466458	-0.038811	1.083244
214.879944	346.191205	4.471462	-0.039355	1.096463
216.688569	355.821334	4.476467	-0.039698	1.109438
219.228132	365.218339	4.481472	-0.040177	1.122123
222.256999	374.451393	4.486477	-0.040747	1.134564
224.324344	383.812628	4.491482	-0.041138	1.146822
226.822764	393.010589	4.496486	-0.041609	1.158839
229.065071	402.178408	4.501491	-0.042033	1.170639
231.983722	411.149236	4.506496	-0.042582	1.182221
235.012391	420.067932	4.511501	-0.043152	1.193649
237.047019	429.124806	4.516506	-0.043537	1.204930
238.976594	438.128616	4.521510	-0.043902	1.216021
240.930197	447.071208	4.526515	-0.044271	1.226944
242.604691	456.004008	4.531520	-0.044589	1.237703
243.238601	465.037592	4.536525	-0.044713	1.248282
244.723316	473.872734	4.541530	-0.044995	1.258709
246.018291	482.681149	4.546534	-0.045242	1.268982
247.792983	491.370186	4.551539	-0.045578	1.279130
249.401195	500.056048	4.556544	-0.045883	1.289162
251.069631	508.683801	4.561549	-0.046199	1.299062
253.067958	517.281084	4.566554	-0.046577	1.308915
254.556152	525.952804	4.571558	-0.046860	1.318680
255.248716	534.650936	4.576563	-0.046994	1.328258
256.968311	543.130939	4.581568	-0.047320	1.337716
258.175092	551.672736	4.586573	-0.047550	1.347082
259.619879	560.171437	4.591578	-0.047825	1.356379
260.625724	568.696916	4.596582	-0.048018	1.365564
261.835035	577.182223	4.601587	-0.048248	1.374680
262.292440	585.776162	4.606592	-0.048339	1.383718
262.829851	594.311606	4.611597	-0.048445	1.392650
264.004154	602.701496	4.616602	-0.048669	1.401485
265.120383	611.089347	4.621606	-0.048882	1.410252
266.609217	619.413660	4.626611	-0.049165	1.418962
268.512829	627.676433	4.631616	-0.049524	1.427626
268.837602	636.192800	4.636621	-0.049590	1.436230
270.276849	644.477958	4.641626	-0.049864	1.444735
270.846199	652.929906	4.646630	-0.049975	1.453212
271.617161	661.309880	4.651635	-0.050124	1.461603
272.354772	669.712391	4.656640	-0.050267	1.469961
273.509641	677.988736	4.661645	-0.050488	1.478216
274.880493	686.218969	4.666650	-0.050748	1.486415
275.343031	694.626267	4.671654	-0.050840	1.494595
276.071654	702.947209	4.676659	-0.050981	1.502689
276.834190	711.272081	4.681664	-0.051128	1.510749
277.680800	719.551065	4.686669	-0.051291	1.518735
278.753732	727.794135	4.691674	-0.051496	1.526680
279.353660	736.139871	4.696678	-0.051613	1.534608
280.045591	744.435058	4.701683	-0.051748	1.542461
280.974612	752.686477	4.706688	-0.051926	1.550270
281.560719	760.969279	4.711693	-0.052040	1.558016
282.450127	769.213521	4.716698	-0.052211	1.565734
282.925604	777.531991	4.721702	-0.052305	1.573420
283.854940	785.708560	4.726707	-0.052484	1.581007
285.032849	793.906703	4.731712	-0.052708	1.588612
286.481222	802.024337	4.736717	-0.052983	1.596148
287.904869	810.185720	4.741722	-0.053254	1.603683
288.911213	818.433959	4.746726	-0.053446	1.611200
290.700003	826.545559	4.751731	-0.053785	1.618672
291.929098	834.775156	4.756736	-0.054019	1.626134
292.942264	843.050189	4.761741	-0.054213	1.633571
294.455201	851.179764	4.766746	-0.054500	1.640917
295.269845	859.437523	4.771750	-0.054657	1.648244
296.156288	867.690603	4.776755	-0.054827	1.655544
297.599187	875.830555	4.781760	-0.055101	1.662790
298.039725	884.146217	4.786765	-0.055189	1.670019
299.372508	892.294924	4.791770	-0.055442	1.677194
299.672813	900.593673	4.796774	-0.055504	1.684327
300.878744	908.749925	4.801779	-0.055733	1.691431
302.258393	916.884229	4.806784	-0.055996	1.698509
302.557120	925.177543	4.811789	-0.056057	1.705547
302.823847	933.511461	4.816794	-0.056112	1.712586
304.021162	941.599112	4.821798	-0.056340	1.719513
304.433651	949.829775	4.826803	-0.056422	1.726428
305.231820	958.026484	4.831808	-0.056576	1.733337
305.747874	966.218977	4.836813	-0.056677	1.740179
306.471673	974.391191	4.841818	-0.056817	1.747003
307.313244	982.552719	4.846822	-0.056979	1.753808
308.360976	990.645308	4.851827	-0.057180	1.760555
309.142187	998.836647	4.856832	-0.057331	1.767323
309.425544	1007.090064	4.861837	-0.057389	1.774053
310.368577	1015.222982	4.866842	-0.057570	1.780742
310.994100	1023.411801	4.871846	-0.057691	1.787412
311.316339	1031.656568	4.876851	-0.057757	1.794063
311.874210	1039.810362	4.881856	-0.057866	1.800646
312.534741	1047.944866	4.886861	-0.057994	1.807203
313.233307	1056.095807	4.891866	-0.058129	1.813753
313.667609	1064.261976	4.896870	-0.058216	1.820260
314.646302	1072.341371	4.901875	-0.058403	1.826740
315.494864	1080.481651	4.906880	-0.058566	1.833230
315.665520	1088.696427	4.911885	-0.058604	1.839673
316.127695	1096.863237	4.916890	-0.058695	1.846091
316.915271	1104.979937	4.921894	-0.058847	1.852487
317.126651	1113.176268	4.926899	-0.058891	1.858853
317.193306	1121.419249	4.931904	-0.058909	1.865217
317.891671	1129.515051	4.936909	-0.059045	1.871520
318.789933	1137.572737	4.941914	-0.059217	1.877796
319.742356	1145.635211	4.946918	-0.059400	1.884061
320.411934	1153.752086	4.951923	-0.059530	1.890313
320.966116	1161.919604	4.956928	-0.059638	1.896569
321.594733	1170.032750	4.961933	-0.059760	1.902773
321.933471	1178.226941	4.966938	-0.059829	1.908983
322.658254	1186.319844	4.971942	-0.059969	1.915142
323.294898	1194.415207	4.976947	-0.060093	1.921272
323.828560	1202.577112	4.981952	-0.060197	1.927421
324.194146	1210.750174	4.986957	-0.060271	1.933539
324.410060	1218.923534	4.991962	-0.060316	1.939622
324.832165	1227.041555	4.996966	-0.060400	1.945667
325.403313	1235.159398	5.001971	-0.060512	1.951710
326.301463	1243.204181	5.006976	-0.060684	1.957717
326.802827	1251.304746	5.011981	-0.060783	1.963702
327.194905	1259.446212	5.016986	-0.060861	1.969687
327.823474	1267.565806	5.021990	-0.060983	1.975663
328.669681	1275.615517	5.026995	-0.061146	1.981594
329.348538	1283.738625	5.032000	-0.061278	1.987542
330.235924	1291.819807	5.037005	-0.061448	1.993464
330.885357	1299.921417	5.042010	-0.061575	1.999358
331.076013	1308.103049	5.047014	-0.061615	2.005243
332.008987	1316.160851	5.052019	-0.061794	2.011100
332.631780	1324.298804	5.057024	-0.061916	2.016965
333.277739	1332.382524	5.062029	-0.062041	2.022776
333.920699	1340.507258	5.067034	-0.062166	2.028600
334.784389	1348.591872	5.072038	-0.062332	2.034401
335.324997	1356.700221	5.077043	-0.062438	2.040168
336.010850	1364.808139	5.082048	-0.062571	2.045934
336.647642	1372.906103	5.087053	-0.062695	2.051672
337.161281	1381.047597	5.092058	-0.062796	2.057411
337.416106	1389.181766	5.097062	-0.062848	2.063102
337.696928	1397.328512	5.102067	-0.062906	2.068789
338.640015	1405.363587	5.107072	-0.063087	2.074450
338.928335	1413.493717	5.112077	-0.063146	2.080095
339.238586	1421.623242	5.117082	-0.063209	2.085727
340.161578	1429.673681	5.122086	-0.063386	2.091350
340.787956	1437.745428	5.127091	-0.063508	2.096943
341.608133	1445.821831	5.132096	-0.063666	2.102543
342.120709	1453.937764	5.137101	-0.063767	2.108125
342.794667	1462.060983	5.142106	-0.063897	2.113712
343.165728	1470.181585	5.147110	-0.063972	2.119254
343.392776	1478.272888	5.152115	-0.064019	2.124747
343.999671	1486.379651	5.157120	-0.064137	2.130273
344.132884	1494.520895	5.162125	-0.064168	2.135761
344.352781	1502.634385	5.167130	-0.064214	2.141226
345.039671	1510.693039	5.172134	-0.064347	2.146684
344.906897	1518.877954	5.177139	-0.064327	2.152135
345.371952	1526.940349	5.182144	-0.064419	2.157547
345.946669	1534.959181	5.187149	-0.064531	2.162927
347.067400	1542.943989	5.192154	-0.064745	2.168323
347.242704	1551.118291	5.197158	-0.064783	2.173740
347.715614	1559.182039	5.202163	-0.064877	2.179100
348.074718	1567.298369	5.207168	-0.064949	2.184470
348.521409	1575.412976	5.212173	-0.065037	2.189834
348.882701	1583.510501	5.217178	-0.065110	2.195166
349.674054	1591.513887	5.222182	-0.065262	2.200463
350.461929	1599.515325	5.227187	-0.065414	2.205745
351.057114	1607.629457	5.232192	-0.065530	2.211070
351.337085	1615.757439	5.237197	-0.065588	2.216362
351.668916	1623.866329	5.242202	-0.065655	2.221634
352.344644	1631.917986	5.247206	-0.065786	2.226888
352.630736	1640.041006	5.252211	-0.065844	2.232140
353.702065	1648.031059	5.257216	-0.066049	2.237365
353.949052	1656.136574	5.262221	-0.066100	2.242577
354.209882	1664.268988	5.267226	-0.066154	2.247796
354.751837	1672.344193	5.272230	-0.066260	2.252991
354.918975	1680.478701	5.277235	-0.066297	2.258178
355.139231	1688.579073	5.282240	-0.066343	2.263337
355.753979	1696.635548	5.287245	-0.066463	2.268490
356.215730	1704.743687	5.292250	-0.066554	2.273651
356.865438	1712.759438	5.297254	-0.066680	2.278759
357.150026	1720.825591	5.302259	-0.066738	2.283854
357.690388	1728.892022	5.307264	-0.066844	2.288961
358.000304	1736.997215	5.312269	-0.066907	2.294060
358.059746	1745.115191	5.317274	-0.066923	2.299135
358.659052	1753.144676	5.322278	-0.067040	2.304189
359.310230	1761.174529	5.327283	-0.067167	2.309237
359.630423	1769.292827	5.332288	-0.067231	2.314301
360.001630	1777.334538	5.337293	-0.067306	2.319310
360.308418	1785.412848	5.342298	-0.067368	2.324326
360.731262	1793.499549	5.347302	-0.067452	2.329345
360.972379	1801.582826	5.352307	-0.067502	2.334336
361.612842	1809.642612	5.357312	-0.067627	2.339336
361.366402	1817.802604	5.362317	-0.067586	2.344312
361.871385	1825.827206	5.367322	-0.067685	2.349258
361.887110	1833.972930	5.372326	-0.067694	2.354226
362.636688	1841.920548	5.377331	-0.067838	2.359124
363.133937	1849.969292	5.382336	-0.067936	2.364052
363.106149	1858.106687	5.387341	-0.067936	2.368980
363.393030	1866.191400	5.392346	-0.067995	2.373892
363.784959	1874.263364	5.397350	-0.068073	2.378795
364.014480	1882.298865	5.402355	-0.068121	2.383652
364.549138	1890.363208	5.407360	-0.068226	2.388541
364.729120	1898.465737	5.412365	-0.068265	2.393415
365.448463	1906.451524	5.417370	-0.068404	2.398252
365.853626	1914.514809	5.422374	-0.068484	2.403100
366.049653	1922.599012	5.427379	-0.068526	2.407935
366.289634	1930.692687	5.432384	-0.068576	2.412768
367.004948	1938.691786	5.437389	-0.068715	2.417574
367.198230	1946.796782	5.442394	-0.068756	2.422391
367.397725	1954.938101	5.447398	-0.068798	2.427221
367.827515	1962.986323	5.452403	-0.068883	2.432004
367.839032	1971.106615	5.457408	-0.068891	2.436787
368.525938	1979.055996	5.462413	-0.069024	2.441513
368.832043	1987.127457	5.467418	-0.069086	2.446272
369.170204	1995.201812	5.472422	-0.069154	2.451026
368.980279	2003.338078	5.477427	-0.069124	2.455766
369.744805	2011.318653	5.482432	-0.069272	2.460479
369.713352	2019.410404	5.487437	-0.069271	2.465187
370.060106	2027.462658	5.492442	-0.069341	2.469892
370.099887	2035.598970	5.497446	-0.069354	2.474613
369.940433	2043.674583	5.502451	-0.069329	2.479275
370.624687	2051.640328	5.507456	-0.069462	2.483929
371.024785	2059.668779	5.512461	-0.069542	2.488588
371.616276	2067.685740	5.517466	-0.069657	2.493246
371.804089	2075.796362	5.522470	-0.069697	2.497920
372.114155	2083.828782	5.527475	-0.069760	2.502548
372.604695	2091.878294	5.532480	-0.069857	2.507191
372.798352	2099.980895	5.537485	-0.069898	2.511834
373.159829	2108.025435	5.542490	-0.069971	2.516448
373.634518	2116.067635	5.547494	-0.070064	2.521060
373.977608	2124.088730	5.552499	-0.070133	2.525642
374.095032	2132.235178	5.557504	-0.070160	2.530270
374.777983	2140.229091	5.562509	-0.070293	2.534844
375.134373	2148.282491	5.567514	-0.070364	2.539420
375.913753	2156.293208	5.572518	-0.070515	2.543994
376.113761	2164.392849	5.577523	-0.070557	2.548568
376.879304	2172.427537	5.582528	-0.070705	2.553138
377.147424	2180.498115	5.587533	-0.070760	2.557684
377.576026	2188.533801	5.592538	-0.070845	2.562214
378.121167	2196.582047	5.597542	-0.070952	2.566751
378.497273	2204.646424	5.602547	-0.071027	2.571277
378.990542	2212.686858	5.607552	-0.071124	2.575790
379.133940	2220.815145	5.612557	-0.071156	2.580319
379.142734	2228.897377	5.617562	-0.071163	2.584805
379.397806	2236.983509	5.622566	-0.071216	2.589303
379.000608	2245.252067	5.627571	-0.071147	2.593848
379.270932	2253.239394	5.632576	-0.071203	2.598277
379.521667	2261.194788	5.637581	-0.071254	2.602679
380.358029	2269.130530	5.642586	-0.071415	2.607103
380.582061	2277.215113	5.647590	-0.071462	2.611559
381.032138	2285.230735	5.652595	-0.071551	2.615985
381.777027	2293.208066	5.657600	-0.071695	2.620402
382.161202	2301.242477	5.662605	-0.071772	2.624819
382.437825	2309.346116	5.667610	-0.071829	2.629259
382.759889	2317.431316	5.672614	-0.071894	2.633684
382.932549	2325.470082	5.677619	-0.071931	2.638066
383.685598	2333.451732	5.682624	-0.072077	2.642449
383.935760	2341.518386	5.687629	-0.072129	2.646837
384.301900	2349.615482	5.692634	-0.072202	2.651242
384.986093	2357.651275	5.697638	-0.072335	2.655628
385.183347	2365.714219	5.702643	-0.072377	2.659988
385.467439	2373.779870	5.707648	-0.072435	2.664349
385.983442	2381.807261	5.712653	-0.072536	2.668697
386.359451	2389.869249	5.717658	-0.072611	2.673047
386.796221	2397.906853	5.722662	-0.072698	2.677381
387.009219	2405.947621	5.727667	-0.072743	2.681695
387.470001	2413.995905	5.732672	-0.072834	2.686022
387.456299	2422.113319	5.737677	-0.072836	2.690348
387.558035	2430.198685	5.742682	-0.072861	2.694658
387.771059	2438.239488	5.747686	-0.072905	2.698944
388.574217	2446.155913	5.752691	-0.073060	2.703195
388.968349	2454.249665	5.757696	-0.073139	2.707507
389.206600	2462.328663	5.762701	-0.073188	2.711795
389.323025	2470.416309	5.767706	-0.073215	2.716072
389.837127	2478.432872	5.772710	-0.073316	2.720330
390.463271	2486.377040	5.777715	-0.073438	2.724551
390.680805	2494.476744	5.782720	-0.073484	2.728821
391.173609	2502.515287	5.787725	-0.073581	2.733069
391.298149	2510.589689	5.792730	-0.073609	2.737307
391.862485	2518.640432	5.797734	-0.073719	2.741553
391.892373	2526.691554	5.802739	-0.073730	2.745759
392.575604	2534.725428	5.807744	-0.073863	2.749990
392.380338	2542.897794	5.812749	-0.073832	2.754233
392.453383	2550.924086	5.817754	-0.073850	2.758410
392.943071	2558.902542	5.822758	-0.073947	2.762581
393.292658	2566.908659	5.827763	-0.074017	2.766751
393.722492	2574.996715	5.832768	-0.074102	2.770962
393.868985	2583.071367	5.837773	-0.074135	2.775143
394.378742	2591.034507	5.842778	-0.074235	2.779282
395.290265	2599.008242	5.847782	-0.074410	2.783444
395.424407	2607.071375	5.852787	-0.074440	2.787599
395.667624	2615.161266	5.857792	-0.074491	2.791768
395.968078	2623.230525	5.862797	-0.074552	2.795924
396.009350	2631.300021	5.867802	-0.074565	2.800058
396.533819	2639.303958	5.872806	-0.074668	2.804181
396.718047	2647.375959	5.877811	-0.074707	2.808313
397.172204	2655.408484	5.882816	-0.074797	2.812434
397.043189	2663.522292	5.887821	-0.074778	2.816557
397.214530	2671.548726	5.892826	-0.074815	2.820646
397.815418	2679.545440	5.897830	-0.074932	2.824740
397.922695	2687.626883	5.902835	-0.074958	2.828841
398.465785	2695.632438	5.907840	-0.075064	2.832924
398.747942	2703.674805	5.912845	-0.075122	2.837004
398.789739	2711.751456	5.917850	-0.075135	2.841082
398.869289	2719.798227	5.922854	-0.075155	2.845141
398.910996	2727.855886	5.927859	-0.075168	2.849197
399.604420	2735.844049	5.932864	-0.075302	2.853250
399.731391	2743.912677	5.937869	-0.075331	2.857305
400.128887	2751.913521	5.942874	-0.075410	2.861336
400.653227	2759.931496	5.947878	-0.075513	2.865377
400.680422	2768.011022	5.952883	-0.075523	2.869415
400.604706	2776.129218	5.957888	-0.075514	2.873460
401.777595	2783.972689	5.962893	-0.075738	2.877433
402.128854	2792.039983	5.967898	-0.075808	2.881466
402.203543	2800.150451	5.972902	-0.075828	2.885499
402.168438	2808.222896	5.977907	-0.075826	2.889501
402.728687	2816.236149	5.982912	-0.075936	2.893502
403.291613	2824.240297	5.987917	-0.076046	2.897492
403.318639	2832.308566	5.992922	-0.076056	2.901479
404.081787	2840.308590	5.997926	-0.076203	2.905468
404.268580	2848.381503	6.002931	-0.076243	2.909455
404.177830	2856.580834	6.007936	-0.076232	2.913483
404.309298	2864.599627	6.012941	-0.076262	2.917430
404.988305	2872.507737	6.017946	-0.076393	2.921347
405.152681	2880.577957	6.022950	-0.076429	2.925309
405.382243	2888.594573	6.027955	-0.076477	2.929244
405.614983	2896.653720	6.032960	-0.076525	2.933194
406.450738	2904.628268	6.037965	-0.076686	2.937130
406.159093	2912.754724	6.042970	-0.076637	2.941074
406.540013	2920.768356	6.047974	-0.076713	2.944994
406.858710	2928.790023	6.052979	-0.076778	2.948910
407.421807	2936.835178	6.057984	-0.076888	2.952844
407.961782	2944.832655	6.062989	-0.076994	2.956749
408.475174	2952.820003	6.067994	-0.077094	2.960642
408.860663	2960.883057	6.072998	-0.077172	2.964560
408.898627	2968.962209	6.078003	-0.077184	2.968462
409.102087	2977.048414	6.083008	-0.077227	2.972371
409.406526	2985.094274	6.088013	-0.077289	2.976261
408.822801	2993.226844	6.093018	-0.077185	2.980141
409.332700	3001.186621	6.098022	-0.077286	2.983990
409.934895	3009.154227	6.103027	-0.077403	2.987842
410.107895	3017.245523	6.108032	-0.077440	2.991726
410.577493	3025.260261	6.113037	-0.077533	2.995584
410.658007	3033.270808	6.118042	-0.077553	2.999415
411.122845	3041.305770	6.123046	-0.077645	3.003273
411.644627	3049.283641	6.128051	-0.077747	3.007100
411.732735	3057.392751	6.133056	-0.077769	3.010964
412.152768	3065.414122	6.138061	-0.077852	3.014797
411.925994	3073.494473	6.143066	-0.077815	3.018622
412.616832	3081.480354	6.148070	-0.077949	3.022442
412.632835	3089.561547	6.153075	-0.077957	3.026269
412.763875	3097.605232	6.158080	-0.077987	3.030079
412.988042	3105.651343	6.163085	-0.078034	3.033890
413.192207	3113.663426	6.168090	-0.078077	3.037679
413.467392	3121.714022	6.173094	-0.078134	3.041485
413.482601	3129.737538	6.178099	-0.078142	3.045261
413.800943	3137.770743	6.183104	-0.078206	3.049051
414.225104	3145.810455	6.188109	-0.078290	3.052845
414.244940	3153.866969	6.193114	-0.078299	3.056623
414.636618	3161.905686	6.198118	-0.078377	3.060405
414.946613	3169.876135	6.203123	-0.078440	3.064147
415.038407	3177.979985	6.208128	-0.078463	3.067936
415.551501	3186.007719	6.213133	-0.078563	3.071704
416.273958	3194.001968	6.218138	-0.078703	3.075463
416.176863	3202.090333	6.223142	-0.078690	3.079222
416.494804	3210.066104	6.228147	-0.078755	3.082943
416.706028	3218.119784	6.233152	-0.078799	3.086691
416.851362	3226.181320	6.238157	-0.078832	3.090435
417.149172	3234.175140	6.243162	-0.078892	3.094150
417.333424	3242.217946	6.248166	-0.078932	3.097878
417.455784	3250.271398	6.253171	-0.078960	3.101603
417.473020	3258.329655	6.258176	-0.078968	3.105322
417.745629	3266.360299	6.263181	-0.079024	3.109035
417.958048	3274.394532	6.268186	-0.079069	3.112742
418.518988	3282.382370	6.273190	-0.079179	3.116440
418.291317	3290.449554	6.278195	-0.079141	3.120133
419.088172	3298.355516	6.283200	-0.079295	3.123795
419.755650	3306.413675	6.288205	-0.079424	3.127517
419.805935	3314.505761	6.293210	-0.079439	3.131221
420.486416	3322.501684	6.298214	-0.079571	3.134906
421.031932	3330.480388	6.303219	-0.079678	3.138572
421.493413	3338.523632	6.308224	-0.079769	3.142259
421.678750	3346.615546	6.313229	-0.079809	3.145952
421.946399	3354.648496	6.318234	-0.079864	3.149617
422.217559	3362.733925	6.323238	-0.079919	3.153302
422.062201	3370.814438	6.328243	-0.079896	3.156961
422.542745	3378.800495	6.333248	-0.079990	3.160602
422.909556	3386.780924	6.338253	-0.080064	3.164231
422.632584	3394.884064	6.343258	-0.080018	3.167882
423.557785	3402.864630	6.348262	-0.080195	3.171527
423.759737	3410.895480	6.353267	-0.080238	3.175159
424.203911	3418.898234	6.358272	-0.080326	3.178784
424.413832	3426.972630	6.363277	-0.080370	3.182427
424.461587	3435.016491	6.368282	-0.080384	3.186045
424.968631	3443.021002	6.373286	-0.080484	3.189661
425.113444	3451.089266	6.378291	-0.080516	3.193286
425.722964	3459.052359	6.383296	-0.080635	3.196880
426.241516	3467.085111	6.388301	-0.080736	3.200497
426.196301	3475.096653	6.393306	-0.080733	3.204076
426.697022	3483.148910	6.398310	-0.080832	3.207692
426.803490	3491.229209	6.403315	-0.080857	3.211300
426.921016	3499.286748	6.408320	-0.080884	3.214895
427.286299	3507.291926	6.413325	-0.080957	3.218472
427.442079	3515.333088	6.418330	-0.080991	3.222053
427.949193	3523.362706	6.423334	-0.081091	3.225639
427.842587	3531.443964	6.428339	-0.081076	3.229218
428.063600	3539.463082	6.433344	-0.081123	3.232780
428.515128	3547.468075	6.438349	-0.081212	3.236341
428.772060	3555.441715	6.443354	-0.081265	3.239876
429.050045	3563.485901	6.448358	-0.081322	3.243439
429.330000	3571.498521	6.453363	-0.081379	3.246985
429.790958	3579.526566	6.458368	-0.081470	3.250540
429.717897	3587.634617	6.463373	-0.081462	3.254105
429.607375	3595.689632	6.468378	-0.081447	3.257642
430.046382	3603.671848	6.473382	-0.081533	3.261164
430.367759	3611.638898	6.478387	-0.081598	3.264672
430.458445	3619.700127	6.483392	-0.081621	3.268208
430.859107	3627.754447	6.488397	-0.081700	3.271749
431.208303	3635.767410	6.493402	-0.081771	3.275266
431.741072	3643.735142	6.498406	-0.081875	3.278767
431.841110	3651.811389	6.503411	-0.081899	3.282294
432.126039	3659.855131	6.508416	-0.081957	3.285811
432.392739	3667.889923	6.513421	-0.082012	3.289319
432.206607	3675.975306	6.518426	-0.081983	3.292828
432.793891	3683.989018	6.523430	-0.082097	3.296332
433.017854	3691.988279	6.528435	-0.082144	3.299812
432.901368	3700.018195	6.533440	-0.082128	3.303288
433.171495	3708.106809	6.538445	-0.082183	3.306801
433.462823	3716.111263	6.543450	-0.082243	3.310274
434.042234	3724.106380	6.548454	-0.082356	3.313751
434.343466	3732.117715	6.553459	-0.082417	3.317221
434.542119	3740.200365	6.558464	-0.082459	3.320713
434.971628	3748.126730	6.563469	-0.082544	3.324144
435.128123	3756.188140	6.568474	-0.082579	3.327618
435.319157	3764.276797	6.573478	-0.082619	3.331102
435.416772	3772.311724	6.578483	-0.082643	3.334555
435.483692	3780.343909	6.583488	-0.082661	3.338003
436.006429	3788.348632	6.588493	-0.082763	3.341453
436.276332	3796.314064	6.593498	-0.082818	3.344872
436.615162	3804.399351	6.598502	-0.082887	3.348342
436.774197	3812.431421	6.603507	-0.082922	3.351779
437.027588	3820.443809	6.608512	-0.082974	3.355207
437.061194	3828.518122	6.613517	-0.082986	3.358650
437.184272	3836.515937	6.618522	-0.083014	3.362060
438.070174	3844.474832	6.623526	-0.083184	3.365478
438.157804	3852.540771	6.628531	-0.083205	3.368909
438.324205	3860.586102	6.633536	-0.083242	3.372330
438.640174	3868.661417	6.638541	-0.083306	3.375767
438.743623	3876.646160	6.643546	-0.083330	3.379153
439.046503	3884.673522	6.648550	-0.083392	3.382561
439.084171	3892.747351	6.653555	-0.083404	3.385976
439.118363	3900.788977	6.658560	-0.083415	3.389374
439.882858	3908.786087	6.663565	-0.083563	3.392776
439.551979	3916.894355	6.668570	-0.083507	3.396181
439.894141	3924.858573	6.673574	-0.083576	3.399547
440.194569	3932.845523	6.678579	-0.083637	3.402918
440.206985	3940.903509	6.683584	-0.083644	3.406304
440.727904	3948.903627	6.688589	-0.083746	3.409681
440.690689	3956.957348	6.693594	-0.083745	3.413058
441.105346	3964.987856	6.698598	-0.083827	3.416437
441.368796	3972.970512	6.703603	-0.083881	3.419788
441.605279	3980.993258	6.708608	-0.083931	3.423151
442.033239	3989.047699	6.713613	-0.084016	3.426530
442.173212	3997.054137	6.718618	-0.084047	3.429876
442.134153	4005.133500	6.723622	-0.084045	3.433244
442.412888	4013.127765	6.728627	-0.084102	3.436583
443.053673	4021.088073	6.733632	-0.084226	3.439917
443.064303	4029.162364	6.738637	-0.084234	3.443274
443.272629	4037.190711	6.743642	-0.084278	3.446615
443.504167	4045.219029	6.748646	-0.084326	3.449954
443.784223	4053.277653	6.753651	-0.084383	3.453303
443.635040	4061.367908	6.758656	-0.084361	3.456648
443.899671	4069.357540	6.763661	-0.084415	3.459962
444.240846	4077.349510	6.768666	-0.084484	3.463277
444.672853	4085.348005	6.773670	-0.084570	3.466593
444.915165	4093.396943	6.778675	-0.084620	3.469921
445.313679	4101.398704	6.783680	-0.084699	3.473232
445.849567	4109.418503	6.788685	-0.084804	3.476551
445.659174	4117.486193	6.793690	-0.084774	3.479863
446.068840	4125.475513	6.798694	-0.084855	3.483159
446.254950	4133.504122	6.803699	-0.084895	3.486461
446.710765	4141.496895	6.808704	-0.084985	3.489754
446.773357	4149.605634	6.813709	-0.085002	3.493078
446.768244	4157.671789	6.818714	-0.085007	3.496380
446.770787	4165.676226	6.823718	-0.085012	3.499653
447.538689	4173.605715	6.828723	-0.085160	3.502918
447.788764	4181.652518	6.833728	-0.085212	3.506210
448.373780	4189.647823	6.838733	-0.085326	3.509489
448.404985	4197.697243	6.843738	-0.085337	3.512769
448.609535	4205.801318	6.848742	-0.085381	3.516074
449.093393	4213.716261	6.853747	-0.085476	3.519308
449.116428	4221.764421	6.858752	-0.085485	3.522578
449.707374	4229.832307	6.863757	-0.085601	3.525872
449.813615	4237.835280	6.868762	-0.085626	3.529120
450.092179	4245.901035	6.873766	-0.085683	3.532396
450.293176	4253.972654	6.878771	-0.085725	3.535669
450.511704	4261.945457	6.883776	-0.085771	3.538900
450.914938	4269.991175	6.888781	-0.085852	3.542163
450.966882	4278.013237	6.893786	-0.085866	3.545402
451.453033	4286.006561	6.898790	-0.085962	3.548640
451.778648	4294.042848	6.903795	-0.086028	3.551888
452.074143	4302.106773	6.908800	-0.086088	3.555142
452.058758	4310.128668	6.913805	-0.086091	3.558368
451.813707	4318.183672	6.918810	-0.086050	3.561597
452.578979	4326.071242	6.923814	-0.086198	3.564786
452.227161	4334.211060	6.928819	-0.086138	3.568039
452.846489	4342.178859	6.933824	-0.086258	3.571250
453.013168	4350.204987	6.938829	-0.086294	3.574468
453.310974	4358.237285	6.943834	-0.086355	3.577690
453.612404	4366.282168	6.948838	-0.086416	3.580913
453.897745	4374.237836	6.953843	-0.086475	3.584097
454.362359	4382.247023	6.958848	-0.086566	3.587306
454.535389	4390.344592	6.963853	-0.086604	3.590538
454.955721	4398.325513	6.968858	-0.086687	3.593727
455.180263	4406.361797	6.973862	-0.086734	3.596930
455.015943	4414.450200	6.978867	-0.086709	3.600140
455.610561	4422.396978	6.983872	-0.086825	3.603313
455.786415	4430.466426	6.988877	-0.086863	3.606519
456.153915	4438.437088	6.993882	-0.086936	3.609689
456.343507	4446.488489	6.998886	-0.086977	3.612883
456.551167	4454.557650	7.003891	-0.087021	3.616081
456.451299	4462.584999	7.008896	-0.087007	3.619252
456.985656	4470.592970	7.013901	-0.087112	3.622429
457.524176	4478.549353	7.018906	-0.087218	3.625584
457.722051	4486.599731	7.023910	-0.087260	3.628764
457.622712	4494.730680	7.028915	-0.087246	3.631964
458.119053	4502.671872	7.033920	-0.087344	3.635103
458.506701	4510.679457	7.038925	-0.087421	3.638262
458.782830	4518.677383	7.043930	-0.087478	3.641412
458.701340	4526.753603	7.048934	-0.087468	3.644580
458.820988	4534.803636	7.053939	-0.087496	3.647740
459.452061	4542.769241	7.058944	-0.087618	3.650879
459.746980	4550.802871	7.063949	-0.087678	3.654032
459.823968	4558.840331	7.068954	-0.087698	3.657178
460.168248	4566.858274	7.073958	-0.087767	3.660321
460.422059	4574.885512	7.078963	-0.087820	3.663463
460.608434	4582.897980	7.083968	-0.087860	3.666594
461.217210	4590.916463	7.088973	-0.087978	3.669736
460.829703	4599.013437	7.093978	-0.087911	3.672879
461.245625	4607.056778	7.098982	-0.087994	3.676020
461.514264	4614.979036	7.103987	-0.088049	3.679107
461.633198	4623.023548	7.108992	-0.088076	3.682235
462.046644	4631.040567	7.113997	-0.088159	3.685358
462.596829	4639.017509	7.119002	-0.088266	3.688466
463.024899	4647.078155	7.124006	-0.088351	3.691601
462.779730	4655.136915	7.129011	-0.088311	3.694714
463.066485	4663.153102	7.134016	-0.088369	3.697822
463.528554	4671.185500	7.139021	-0.088461	3.700939
463.411406	4679.209977	7.144026	-0.088444	3.704035
463.838970	4687.250376	7.149030	-0.088529	3.707148
463.486927	4695.364607	7.154035	-0.088469	3.710267
463.670882	4703.365087	7.159040	-0.088508	3.713353
464.455376	4711.329644	7.164045	-0.088659	3.716439
464.992853	4719.269422	7.169050	-0.088765	3.719505
465.151466	4727.309816	7.174054	-0.088799	3.722599
465.692986	4735.292199	7.179059	-0.088905	3.725677
465.842617	4743.338606	7.184064	-0.088938	3.728767
465.806196	4751.457578	7.189069	-0.088937	3.731877
465.883396	4759.449571	7.194074	-0.088956	3.734940
466.401149	4767.441071	7.199078	-0.089058	3.738010
466.650676	4775.524374	7.204083	-0.089110	3.741107
467.223442	4783.382074	7.209088	-0.089221	3.744122
467.275333	4791.524215	7.214093	-0.089236	3.747231
467.532149	4799.561039	7.219098	-0.089289	3.750302
467.989892	4807.541855	7.224102	-0.089380	3.753354
467.988709	4815.637907	7.229107	-0.089385	3.756437
468.385328	4823.537431	7.234112	-0.089464	3.759451
468.711107	4831.601574	7.239117	-0.089530	3.762524
468.965650	4839.614415	7.244122	-0.089582	3.765574
469.062109	4847.657713	7.249126	-0.089606	3.768628
468.988952	4855.778253	7.254131	-0.089597	3.771706
469.309680	4863.713661	7.259136	-0.089662	3.774719
469.554680	4871.773264	7.264141	-0.089713	3.777776
469.367010	4879.841363	7.269146	-0.089683	3.780824
470.010216	4887.738494	7.274150	-0.089808	3.783823
470.477117	4895.782806	7.279155	-0.089900	3.786872
470.740248	4903.796570	7.284160	-0.089954	3.789902
471.436453	4911.836122	7.289165	-0.090089	3.792949
471.655307	4919.880684	7.294170	-0.090135	3.795984
471.823203	4927.858528	7.299174	-0.090172	3.798991
472.222311	4935.945119	7.304179	-0.090251	3.802042
472.718754	4943.872154	7.309184	-0.090349	3.805032
472.444320	4952.013911	7.314189	-0.090303	3.808083
472.190066	4960.093458	7.319194	-0.090261	3.811109
472.122391	4968.069944	7.324198	-0.090253	3.814098
472.626941	4976.076322	7.329203	-0.090353	3.817108
472.577078	4984.068553	7.334208	-0.090349	3.820099
473.093225	4992.084691	7.339213	-0.090450	3.823109
473.490830	5000.061676	7.344218	-0.090529	3.826099
473.496778	5008.111445	7.349222	-0.090535	3.829105
474.074741	5016.176107	7.354227	-0.090648	3.832127
474.206881	5024.130012	7.359232	-0.090678	3.835095
474.477198	5032.156767	7.364237	-0.090734	3.838091
474.816815	5040.219487	7.369242	-0.090802	3.841100
475.021884	5048.175499	7.374246	-0.090845	3.844064
475.522164	5056.278832	7.379251	-0.090944	3.847086
475.105947	5064.314886	7.384256	-0.090871	3.850062
475.657584	5072.296081	7.389261	-0.090979	3.853035
475.558085	5080.382899	7.394266	-0.090966	3.856031
475.952187	5088.357915	7.399270	-0.091045	3.858995
476.186673	5096.397145	7.404275	-0.091094	3.861976
476.016137	5104.405458	7.409280	-0.091067	3.864935
476.641476	5112.407489	7.414285	-0.091189	3.867906
476.945425	5120.421158	7.419290	-0.091250	3.870872
477.071461	5128.577068	7.424294	-0.091279	3.873885
477.220526	5136.590760	7.429299	-0.091312	3.876843
477.713995	5144.454377	7.434304	-0.091409	3.879751
478.068789	5152.507294	7.439309	-0.091480	3.882723
478.104569	5160.506745	7.444314	-0.091492	3.885667
478.756692	5168.476151	7.449318	-0.091619	3.888610
479.187375	5176.538720	7.454323	-0.091704	3.891581
479.467298	5184.515405	7.459328	-0.091762	3.894515
480.152963	5192.557251	7.464333	-0.091894	3.897478
480.448983	5200.531011	7.469338	-0.091955	3.900407
480.604907	5208.590878	7.474342	-0.091989	3.903362
480.570703	5216.690104	7.479347	-0.091988	3.906325
480.405104	5224.710216	7.484352	-0.091962	3.909255
480.754985	5232.789341	7.489357	-0.092033	3.912214
481.070569	5240.772199	7.494362	-0.092097	3.915135
481.522446	5248.737738	7.499366	-0.092186	3.918050
482.117336	5256.711348	7.504371	-0.092302	3.920968
482.017284	5264.761685	7.509376	-0.092288	3.923899
481.981222	5272.867873	7.514381	-0.092287	3.926849
482.493085	5280.820435	7.519386	-0.092387	3.929752
482.745534	5288.877538	7.524390	-0.092440	3.932685
483.271795	5296.893177	7.529395	-0.092543	3.935607
483.324831	5304.887583	7.534400	-0.092558	3.938509
484.300977	5312.856375	7.539405	-0.092745	3.941417
485.006461	5320.804714	7.544410	-0.092881	3.944311
484.520942	5328.970351	7.549414	-0.092796	3.947259
485.070393	5336.992231	7.554419	-0.092904	3.950172
485.398900	5345.010631	7.559424	-0.092970	3.953077
485.647581	5353.051168	7.564429	-0.093022	3.955987
485.921309	5361.031617	7.569434	-0.093078	3.958873
486.261501	5369.079641	7.574438	-0.093146	3.961783
486.832953	5376.998433	7.579443	-0.093258	3.964648
486.269772	5385.122064	7.584448	-0.093158	3.967564
486.764083	5393.149304	7.589453	-0.093256	3.970463
486.913962	5401.184678	7.594458	-0.093289	3.973356
487.404668	5409.164234	7.599462	-0.093385	3.976233
487.968718	5417.161885	7.604467	-0.093496	3.979115
487.600348	5425.210540	7.609472	-0.093432	3.981998
488.187891	5433.187627	7.614477	-0.093547	3.984869
488.376555	5441.189801	7.619482	-0.093587	3.987741
488.951891	5449.226502	7.624486	-0.093699	3.990629
489.165456	5457.255022	7.629491	-0.093744	3.993506
489.209544	5465.306167	7.634496	-0.093758	3.996386
489.245759	5473.316325	7.639501	-0.093770	3.999249
489.560022	5481.347207	7.644506	-0.093833	4.002122
490.137291	5489.280711	7.649510	-0.093946	4.004963
490.530936	5497.371389	7.654515	-0.094025	4.007854
490.527166	5505.397945	7.659520	-0.094029	4.010714
490.204841	5513.494903	7.664525	-0.093974	4.013592
490.367905	5521.505942	7.669530	-0.094010	4.016446
490.664578	5529.442870	7.674534	-0.094070	4.019273
491.372626	5537.496897	7.679539	-0.094207	4.022146
491.147597	5545.475217	7.684544	-0.094171	4.024975
491.756466	5553.497165	7.689549	-0.094289	4.027831
491.724257	5561.595250	7.694554	-0.094289	4.030702
492.238737	5569.578587	7.699558	-0.094390	4.033538
493.081911	5577.589311	7.704563	-0.094552	4.036388
493.173968	5585.543111	7.709568	-0.094574	4.039203
493.343874	5593.635114	7.714573	-0.094611	4.042067
493.607188	5601.567060	7.719578	-0.094665	4.044873
493.721607	5609.628795	7.724582	-0.094692	4.047721
494.065132	5617.667704	7.729587	-0.094761	4.050562
493.748514	5625.780872	7.734592	-0.094707	4.053418
493.676082	5633.858963	7.739597	-0.094699	4.056262
494.339648	5641.717712	7.744602	-0.094828	4.059039
494.555546	5649.783245	7.749606	-0.094873	4.061880
495.010180	5657.709334	7.754611	-0.094963	4.064673
495.205220	5665.761411	7.759616	-0.095004	4.067505
495.163428	5673.872762	7.764621	-0.095002	4.070352
495.953289	5681.800881	7.769626	-0.095154	4.073145
496.520150	5689.803779	7.774630	-0.095265	4.075958
496.583303	5697.886876	7.779635	-0.095282	4.078791
496.329333	5705.960194	7.784640	-0.095240	4.081614
496.916361	5713.874936	7.789645	-0.095354	4.084391
497.392159	5721.907075	7.794650	-0.095448	4.087206
497.792585	5729.901545	7.799654	-0.095528	4.090004
497.609089	5738.004979	7.804659	-0.095499	4.092831
497.987029	5746.001752	7.809664	-0.095574	4.095626
498.324894	5753.995910	7.814669	-0.095642	4.098417
497.681729	5762.127233	7.819674	-0.095528	4.101241
497.881611	5770.067981	7.824678	-0.095570	4.104009
498.562740	5778.043594	7.829683	-0.095702	4.106793
498.877207	5786.031275	7.834688	-0.095766	4.109574
499.059698	5794.090807	7.839693	-0.095805	4.112377
499.038895	5802.148559	7.844698	-0.095807	4.115174
499.227118	5810.127168	7.849702	-0.095847	4.117945
499.774674	5818.166715	7.854707	-0.095954	4.120740
499.692592	5826.112665	7.859712	-0.095944	4.123492
500.009075	5834.212815	7.864717	-0.096008	4.126301
499.926913	5842.196596	7.869722	-0.095998	4.129062
500.348650	5850.225332	7.874726	-0.096082	4.131844
500.736155	5858.213953	7.879731	-0.096159	4.134609
500.649304	5866.264745	7.884736	-0.096148	4.137388
500.940258	5874.278790	7.889741	-0.096208	4.140157
501.305978	5882.263861	7.894746	-0.096281	4.142916
501.223523	5890.316247	7.899750	-0.096271	4.145690
501.131470	5898.401557	7.904755	-0.096259	4.148473
501.525918	5906.397387	7.909760	-0.096337	4.151230
501.880964	5914.348371	7.914765	-0.096409	4.153969
501.763414	5922.472652	7.919770	-0.096392	4.156759
502.094510	5930.379840	7.924774	-0.096459	4.159479
502.728271	5938.430768	7.929779	-0.096582	4.162250
502.924847	5946.388126	7.934784	-0.096624	4.164982
502.683434	5954.496547	7.939789	-0.096584	4.167758
503.006073	5962.514808	7.944794	-0.096649	4.170509
503.176224	5970.521930	7.949798	-0.096686	4.173252
503.388538	5978.578582	7.954803	-0.096731	4.176010
503.205849	5986.571159	7.959808	-0.096702	4.178741
503.715253	5994.582619	7.964813	-0.096802	4.181484
503.566147	6002.590930	7.969818	-0.096780	4.184216
503.948612	6010.642220	7.974822	-0.096856	4.186967
504.697112	6018.606020	7.979827	-0.097001	4.189691
504.687159	6026.722660	7.984832	-0.097004	4.192457
504.631841	6034.776470	7.989837	-0.096999	4.195199
505.152037	6042.713666	7.994842	-0.097101	4.197905
505.321326	6050.727463	7.999846	-0.097138	4.200632
505.468439	6058.729811	8.004851	-0.097170	4.203354
505.199458	6066.825446	8.009856	-0.097126	4.206100
505.544754	6074.777563	8.014861	-0.097195	4.208803
505.759635	6082.804511	8.019866	-0.097240	4.211528
505.641962	6090.814218	8.024870	-0.097223	4.214241
505.946929	6098.911499	8.029875	-0.097286	4.216987
506.112348	6106.818402	8.034880	-0.097321	4.219666
506.257299	6114.869519	8.039885	-0.097354	4.222391
506.753511	6122.817952	8.044890	-0.097451	4.225083
506.994039	6130.852616	8.049894	-0.097501	4.227800
507.199257	6138.930642	8.054899	-0.097545	4.230530
507.443712	6146.921144	8.059904	-0.097595	4.233229
507.586822	6154.974579	8.064909	-0.097627	4.235946
507.856684	6162.951574	8.069914	-0.097683	4.238637
507.787180	6170.986601	8.074918	-0.097675	4.241342
508.415255	6178.910352	8.079923	-0.097797	4.244015
508.757040	6186.997342	8.084928	-0.097866	4.246738
509.030584	6195.015490	8.089933	-0.097922	4.249436
509.117379	6203.095448	8.094938	-0.097943	4.252151
509.268264	6211.068041	8.099942	-0.097977	4.254829
509.502261	6219.112218	8.104947	-0.098026	4.257529
509.071015	6227.176007	8.109952	-0.097950	4.260229
509.618682	6235.093847	8.114957	-0.098058	4.262887
510.452043	6243.063815	8.119962	-0.098218	4.265563
510.478384	6251.125249	8.124966	-0.098228	4.268261
510.829386	6259.198632	8.129971	-0.098299	4.270964
510.720774	6267.209631	8.134976	-0.098284	4.273640
510.579887	6275.279801	8.139981	-0.098263	4.276334
510.873212	6283.185037	8.144986	-0.098322	4.278975
511.687346	6291.169183	8.149990	-0.098479	4.281646
511.932898	6299.145837	8.154995	-0.098530	4.284307
512.099629	6307.246843	8.160000	-0.098566	4.287007
511.953100	6315.267529	8.165005	-0.098544	4.289676
512.656040	6323.283955	8.170010	-0.098680	4.292350
512.723709	6331.289386	8.175014	-0.098698	4.295012
513.016679	6339.325934	8.180019	-0.098758	4.297685
512.965155	6347.358603	8.185024	-0.098754	4.300352
513.223494	6355.349758	8.190029	-0.098807	4.303007
512.777734	6363.488078	8.195034	-0.098729	4.305702
513.311901	6371.460665	8.200038	-0.098834	4.308349
513.783878	6379.461613	8.205043	-0.098927	4.311004
513.852881	6387.415400	8.210048	-0.098945	4.313637
514.157627	6395.440978	8.215053	-0.099007	4.316295
514.669918	6403.391021	8.220058	-0.099107	4.318928
514.315192	6411.478590	8.225062	-0.099047	4.321598
514.310687	6419.490762	8.230067	-0.099051	4.324244
514.191075	6427.560734	8.235072	-0.099034	4.326906
514.799168	6435.504865	8.240077	-0.099152	4.329531
515.167918	6443.537353	8.245082	-0.099226	4.332182
515.145572	6451.542269	8.250086	-0.099227	4.334818
515.340739	6459.572671	8.255091	-0.099269	4.337464
515.318187	6467.606378	8.260096	-0.099270	4.340107
515.343515	6475.642949	8.265101	-0.099280	4.342749
515.672014	6483.618724	8.270106	-0.099346	4.345373
515.886400	6491.652390	8.275110	-0.099391	4.348013
516.214607	6499.651421	8.280115	-0.099457	4.350641
516.480287	6507.700586	8.285120	-0.099512	4.353283
516.414900	6515.757149	8.290125	-0.099505	4.355923
516.298139	6523.760581	8.295130	-0.099489	4.358545
516.615037	6531.742419	8.300134	-0.099553	4.361160
516.752857	6539.705273	8.305139	-0.099584	4.363767
517.007714	6547.747864	8.310144	-0.099636	4.366399
517.244906	6555.777628	8.315149	-0.099686	4.369025
517.524067	6563.852581	8.320154	-0.099743	4.371664
518.022670	6571.746318	8.325158	-0.099841	4.374244
518.398920	6579.836918	8.330163	-0.099916	4.376886
518.610788	6587.811305	8.335168	-0.099961	4.379487
518.610755	6595.923124	8.340173	-0.099966	4.382130
519.213585	6603.843982	8.345178	-0.100083	4.384713
519.547545	6611.861305	8.350182	-0.100151	4.387325
519.672102	6619.930747	8.355187	-0.100179	4.389950
520.050325	6627.966664	8.360192	-0.100255	4.392564
520.074386	6636.020871	8.365197	-0.100265	4.395181
520.333702	6644.062082	8.370202	-0.100318	4.397793
520.418943	6652.046880	8.375206	-0.100339	4.400384
520.853012	6660.055158	8.380211	-0.100425	4.402984
520.755098	6668.063412	8.385216	-0.100412	4.405578
521.222618	6676.065385	8.390221	-0.100504	4.408173
521.417433	6684.166767	8.395226	-0.100546	4.410796
521.517769	6692.120233	8.400230	-0.100570	4.413370
522.062920	6700.203113	8.405235	-0.100677	4.415986
521.928155	6708.201027	8.410240	-0.100657	4.418569
521.866917	6716.284548	8.415245	-0.100651	4.421179
522.366190	6724.181649	8.420250	-0.100749	4.423731
522.630420	6732.255824	8.425254	-0.100803	4.426336
522.337066	6740.339020	8.430259	-0.100754	4.428940
522.957865	6748.305666	8.435264	-0.100874	4.431510
523.297796	6756.248634	8.440269	-0.100943	4.434069
523.392495	6764.345722	8.445274	-0.100966	4.436675
523.695561	6772.237577	8.450278	-0.101027	4.439214
524.111370	6780.343220	8.455283	-0.101110	4.441822
523.946024	6788.320544	8.460288	-0.101084	4.444383
523.918172	6796.401553	8.465293	-0.101084	4.446977
524.404993	6804.398019	8.470298	-0.101180	4.449545
524.281492	6812.441190	8.475302	-0.101163	4.452124
524.577994	6820.411890	8.480307	-0.101223	4.454679
525.033189	6828.417252	8.485312	-0.101313	4.457245
524.685956	6836.459939	8.490317	-0.101253	4.459818
525.147631	6844.500054	8.495322	-0.101345	4.462392
525.447537	6852.411399	8.500326	-0.101406	4.464923
526.069510	6860.461890	8.505331	-0.101527	4.467498
526.181291	6868.528804	8.510336	-0.101553	4.470074
526.049863	6876.576140	8.515341	-0.101533	4.472642
526.391608	6884.584888	8.520346	-0.101602	4.475198
526.762089	6892.542164	8.525350	-0.101676	4.477736
526.613682	6900.575139	8.530355	-0.101654	4.480295
527.075721	6908.556280	8.535360	-0.101745	4.482838
527.250126	6916.590685	8.540365	-0.101783	4.485396
527.293195	6924.633245	8.545370	-0.101796	4.487954
527.064479	6932.647176	8.550374	-0.101759	4.490501
527.578937	6940.667050	8.555379	-0.101860	4.493051
527.639678	6948.690801	8.560384	-0.101876	4.495598
527.685459	6956.662220	8.565389	-0.101890	4.498128
527.780250	6964.733143	8.570394	-0.101913	4.500688
528.390994	6972.653555	8.575399	-0.102032	4.503201
528.556986	6980.726144	8.580403	-0.102068	4.505759
528.563392	6988.749764	8.585408	-0.102074	4.508299
528.709415	6996.809110	8.590413	-0.102107	4.510850
529.218557	7004.790573	8.595418	-0.102207	4.513375
529.143993	7012.774344	8.600423	-0.102198	4.515899
529.815735	7020.707188	8.605427	-0.102328	4.518406
529.664436	7028.833207	8.610432	-0.102305	4.520972
529.141974	7036.789933	8.615437	-0.102213	4.523481
529.856078	7044.820331	8.620442	-0.102351	4.526015
529.620179	7052.850718	8.625447	-0.102313	4.528546
530.251956	7060.869380	8.630451	-0.102435	4.531073
530.309923	7068.892472	8.635456	-0.102451	4.533599
530.310595	7076.922508	8.640461	-0.102457	4.536126
530.868490	7084.882220	8.645466	-0.102566	4.538630
530.932312	7092.908897	8.650471	-0.102583	4.541153
531.127659	7100.948055	8.655475	-0.102625	4.543679
530.910907	7109.016594	8.660480	-0.102589	4.546211
531.188933	7116.966688	8.665485	-0.102646	4.548706
531.047978	7125.086410	8.670490	-0.102625	4.551252
531.551283	7132.984217	8.675495	-0.102724	4.553729
531.682293	7141.096257	8.680499	-0.102754	4.556270
531.816088	7148.951524	8.685504	-0.102784	4.558730
532.784121	7156.962811	8.690509	-0.102969	4.561238
532.435173	7165.061387	8.695514	-0.102910	4.563770
532.419287	7173.091535	8.700519	-0.102912	4.566280
532.939582	7181.060238	8.705523	-0.103014	4.568770
533.688601	7189.085331	8.710528	-0.103159	4.571277
533.369646	7197.147475	8.715533	-0.103104	4.573792
533.845321	7205.170081	8.720538	-0.103198	4.576294
533.856472	7213.140291	8.725543	-0.103205	4.578779
534.168453	7221.194720	8.730547	-0.103269	4.581288
534.300273	7229.165182	8.735552	-0.103298	4.583770
534.696393	7237.207209	8.740557	-0.103377	4.586273
535.076045	7245.238794	8.745562	-0.103453	4.588771
535.141545	7253.280065	8.750567	-0.103471	4.591270
535.624429	7261.248933	8.755571	-0.103566	4.593746
535.672774	7269.326288	8.760576	-0.103580	4.596254
535.903849	7277.232422	8.765581	-0.103628	4.598708
536.251441	7285.321776	8.770586	-0.103698	4.601217
536.107568	7293.317244	8.775591	-0.103677	4.603695
536.102669	7301.367034	8.780595	-0.103681	4.606189
536.222575	7309.343254	8.785600	-0.103708	4.608659
536.301238	7317.381410	8.790605	-0.103728	4.611147
536.690969	7325.362791	8.795610	-0.103806	4.613615
536.910899	7333.384245	8.800615	-0.103852	4.616095
537.135622	7341.368659	8.805619	-0.103899	4.618562
537.053185	7349.445807	8.810624	-0.103889	4.621056
537.162541	7357.457274	8.815629	-0.103915	4.623529
538.000122	7365.449160	8.820634	-0.104076	4.625994
537.952217	7373.480683	8.825639	-0.104072	4.628471
538.862172	7381.468404	8.830643	-0.104247	4.630932
539.250985	7389.442632	8.835648	-0.104324	4.633388
539.519775	7397.501414	8.840653	-0.104380	4.635868
539.575639	7405.541252	8.845658	-0.104395	4.638341
539.384787	7413.590414	8.850663	-0.104365	4.640816
539.872111	7421.518134	8.855667	-0.104461	4.643252
540.152791	7429.578184	8.860672	-0.104518	4.645728
540.164535	7437.543730	8.865677	-0.104526	4.648173
540.457298	7445.624736	8.870682	-0.104585	4.650652
540.344828	7453.675028	8.875687	-0.104570	4.653121
540.431328	7461.704381	8.880691	-0.104591	4.655581
540.473123	7469.692072	8.885696	-0.104604	4.658028
540.185104	7477.718051	8.890701	-0.104556	4.660485
540.546632	7485.688268	8.895706	-0.104628	4.662924
540.547512	7493.703857	8.900711	-0.104633	4.665375
540.950207	7501.768586	8.905715	-0.104714	4.667840
540.754586	7509.788114	8.910720	-0.104682	4.670290
540.475168	7517.871889	8.915725	-0.104636	4.672759
540.964572	7525.818917	8.920730	-0.104732	4.675184
541.256731	7533.788058	8.925735	-0.104791	4.677614
541.393585	7541.817272	8.930739	-0.104822	4.680062
541.608357	7549.830535	8.935744	-0.104867	4.682503
541.705021	7557.755332	8.940749	-0.104890	4.684917
542.070157	7565.847439	8.945754	-0.104964	4.687379
541.347609	7573.904471	8.950759	-0.104834	4.689831
541.895546	7581.924827	8.955763	-0.104942	4.692269
542.406043	7589.878501	8.960768	-0.105042	4.694686
542.756350	7597.851131	8.965773	-0.105112	4.697107
542.676390	7605.909190	8.970778	-0.105103	4.699553
542.999399	7613.941611	8.975783	-0.105168	4.701990
543.068701	7621.929599	8.980787	-0.105186	4.704412
543.409349	7629.981978	8.985792	-0.105255	4.706852
543.479944	7637.929911	8.990797	-0.105273	4.709260
543.740179	7646.067690	8.995802	-0.105327	4.711724
543.802176	7654.032161	9.000807	-0.105343	4.714134
544.267914	7662.064223	9.005811	-0.105435	4.716563
544.398922	7670.027142	9.010816	-0.105465	4.718970
544.534971	7678.106871	9.015821	-0.105496	4.721411
545.080743	7686.057197	9.020826	-0.105602	4.723811
545.328456	7694.104836	9.025831	-0.105654	4.726239
545.824813	7702.071595	9.030835	-0.105751	4.728642
545.331785	7710.226738	9.035840	-0.105665	4.731102
545.301377	7718.214407	9.040845	-0.105664	4.733509
545.751847	7726.222393	9.045850	-0.105753	4.735920
545.948747	7734.162049	9.050855	-0.105795	4.738310
546.203636	7742.225623	9.055859	-0.105848	4.740736
546.570122	7750.216512	9.060864	-0.105921	4.743138
546.993425	7758.231834	9.065869	-0.106005	4.745547
547.502328	7766.266715	9.070874	-0.106105	4.747959
547.355182	7774.298871	9.075879	-0.106083	4.750372
547.969047	7782.345264	9.080883	-0.106203	4.752785
547.774717	7790.385190	9.085888	-0.106172	4.755197
548.046398	7798.261799	9.090893	-0.106227	4.757558
548.350570	7806.361583	9.095898	-0.106289	4.759985
548.066267	7814.388794	9.100903	-0.106241	4.762390
548.268369	7822.354031	9.105907	-0.106284	4.764774
548.445449	7830.447274	9.110912	-0.106323	4.767195
548.333341	7838.409011	9.115917	-0.106307	4.769576
548.787286	7846.457106	9.120922	-0.106397	4.771981
548.780028	7854.462531	9.125927	-0.106400	4.774372
549.427187	7862.428102	9.130931	-0.106526	4.776749
549.691482	7870.468844	9.135936	-0.106580	4.779148
549.490378	7878.497844	9.140941	-0.106548	4.781544
549.916888	7886.450259	9.145946	-0.106633	4.783913
549.983653	7894.549160	9.150951	-0.106651	4.786326
550.193371	7902.509251	9.155955	-0.106695	4.788697
550.329462	7910.592038	9.160960	-0.106725	4.791103
550.323330	7918.530225	9.165965	-0.106729	4.793465
550.745317	7926.606973	9.170970	-0.106813	4.795865
550.789709	7934.526494	9.175975	-0.106827	4.798219
550.729632	7942.652449	9.180979	-0.106821	4.800634
550.756739	7950.644843	9.185984	-0.106831	4.803007
551.138657	7958.582910	9.190989	-0.106907	4.805362
551.431843	7966.722745	9.195994	-0.106967	4.807775
551.171355	7974.667367	9.200999	-0.106924	4.810132
551.523905	7982.687714	9.206003	-0.106995	4.812508
551.969008	7990.088367	9.211008	-0.107082	4.814698
552.186864	7994.854941	9.216013	-0.107126	4.816109

551.788028	7997.550938	9.221018	-0.107053	4.816908
551.942950	7998.861009	9.226023	-0.107083	4.817295
552.261484	7999.279119	9.231027	-0.107143	4.817418
552.363756	8000.482041	9.236032	-0.107162	4.817773
552.028255	8000.471857	9.241037	-0.107100	4.817772
552.172629	8000.424390	9.246042	-0.107127	4.817757
552.878755	8000.449487	9.251047	-0.107258	4.817762
552.709442	8000.488147	9.256051	-0.107227	4.817774
552.899551	8000.487763	9.261056	-0.107262	4.817773
552.922884	8000.456457	9.266061	-0.107266	4.817763
552.721104	8000.310043	9.271066	-0.107229	4.817721
552.556789	8000.447932	9.276071	-0.107198	4.817763
552.579452	8000.488346	9.281075	-0.107202	4.817774
552.539656	8000.424471	9.286080	-0.107195	4.817756
552.976127	8000.470941	9.291085	-0.107276	4.817768
553.070153	8000.481809	9.296090	-0.107294	4.817770
553.017145	8000.390313	9.301095	-0.107284	4.817743
552.730359	8000.458900	9.306099	-0.107230	4.817765
552.454948	8000.316684	9.311104	-0.107179	4.817724
552.424704	8000.353160	9.316109	-0.107173	4.817735
553.165092	8000.379813	9.321114	-0.107311	4.817740
553.210163	8000.545030	9.326119	-0.107320	4.817788
553.089360	8000.361823	9.331123	-0.107297	4.817735
553.166199	8000.328136	9.336128	-0.107311	4.817724
553.572297	8000.399479	9.341133	-0.107387	4.817744
554.027022	8000.500018	9.346138	-0.107472	4.817772
553.582846	8000.520941	9.351143	-0.107389	4.817780
553.574174	8000.412160	9.356147	-0.107387	4.817748
553.455635	8000.435740	9.361152	-0.107365	4.817755
553.417216	8000.442560	9.366157	-0.107358	4.817757
553.388025	8000.357741	9.371162	-0.107352	4.817732
553.394106	8000.345170	9.376167	-0.107354	4.817729
553.242414	8000.319742	9.381171	-0.107325	4.817722
553.354243	8000.334035	9.386176	-0.107346	4.817725
553.394243	8000.346222	9.391181	-0.107353	4.817729
554.083262	8000.453355	9.396186	-0.107482	4.817758
554.410880	8000.477138	9.401191	-0.107543	4.817763
554.008760	8000.473358	9.406195	-0.107468	4.817764
554.091706	8000.431320	9.411200	-0.107483	4.817751
554.423896	8000.450951	9.416205	-0.107545	4.817755
554.815732	8000.450358	9.421210	-0.107618	4.817753
554.983702	8000.487629	9.426215	-0.107649	4.817764
554.772747	8000.507746	9.431219	-0.107610	4.817771
554.591419	8000.416476	9.436224	-0.107576	4.817744
554.397267	8000.501188	9.441229	-0.107540	4.817770
554.794727	8000.405736	9.446234	-0.107614	4.817740
554.738148	8000.526220	9.451239	-0.107604	4.817776
554.775905	8000.520442	9.456243	-0.107611	4.817774
554.799604	8000.399473	9.461248	-0.107615	4.817739
554.594312	8000.433387	9.466253	-0.107577	4.817749
554.662572	8000.455483	9.471258	-0.107589	4.817756
554.865091	8000.472161	9.476263	-0.107627	4.817760
555.123323	8000.484381	9.481267	-0.107675	4.817762
555.397025	8000.477840	9.486272	-0.107726	4.817759
555.502962	8000.468841	9.491277	-0.107746	4.817756
555.375474	8000.489125	9.496282	-0.107722	4.817763
555.061574	8000.385363	9.501287	-0.107663	4.817733
555.248929	8000.497817	9.506291	-0.107698	4.817766
555.261322	8000.508546	9.511296	-0.107701	4.817769
555.353630	8000.456095	9.516301	-0.107718	4.817753
555.522151	8000.515529	9.521306	-0.107749	4.817770
554.990735	8000.431788	9.526311	-0.107650	4.817747
555.062799	8000.414908	9.531315	-0.107664	4.817742
555.805274	8000.503848	9.536320	-0.107802	4.817765
555.544670	8000.472600	9.541325	-0.107753	4.817757
555.597133	8000.516619	9.546330	-0.107763	4.817770
555.669180	8000.459652	9.551335	-0.107776	4.817753
555.666001	8000.398417	9.556339	-0.107776	4.817734
555.647871	8000.521577	9.561344	-0.107772	4.817771
555.919185	8000.493903	9.566349	-0.107823	4.817762
555.669874	8000.439611	9.571354	-0.107776	4.817747
555.815477	8000.430139	9.576359	-0.107804	4.817743
555.883488	8000.508144	9.581363	-0.107816	4.817766
556.172445	8000.499718	9.586368	-0.107870	4.817762
555.942232	8000.467859	9.591373	-0.107827	4.817754
556.000811	8000.501419	9.596378	-0.107838	4.817763
556.166038	8000.469025	9.601383	-0.107869	4.817753
556.001175	8000.494036	9.606387	-0.107838	4.817761
556.132425	8000.483299	9.611392	-0.107862	4.817758
555.332278	8000.426211	9.616397	-0.107713	4.817744
555.738190	8000.445870	9.621402	-0.107789	4.817748
555.688502	8000.513711	9.626407	-0.107780	4.817768
555.942095	8000.488942	9.631411	-0.107827	4.817760
556.296672	8000.400247	9.636416	-0.107893	4.817732
556.173254	8000.470172	9.641421	-0.107870	4.817753
555.948550	8000.511185	9.646426	-0.107828	4.817767
556.250878	8000.499790	9.651431	-0.107884	4.817762
556.234581	8000.518539	9.656435	-0.107881	4.817768
556.053377	8000.421991	9.661440	-0.107847	4.817740
556.177052	8000.479714	9.666445	-0.107871	4.817756
556.242287	8000.407877	9.671450	-0.107883	4.817735
556.588241	8000.492067	9.676455	-0.107947	4.817758
556.631733	8000.509583	9.681459	-0.107955	4.817763
556.511302	8000.504651	9.686464	-0.107933	4.817762
556.291954	8000.467675	9.691469	-0.107892	4.817752
556.001690	8000.511947	9.696474	-0.107838	4.817767
556.175259	8000.476511	9.701479	-0.107870	4.817755
556.411643	8000.488413	9.706483	-0.107914	4.817758
556.414336	8000.515880	9.711488	-0.107915	4.817766
556.317829	8000.487035	9.716493	-0.107897	4.817758
556.282865	8000.420059	9.721498	-0.107890	4.817738
556.566076	8000.481176	9.726503	-0.107943	4.817755
556.461873	8000.495471	9.731507	-0.107923	4.817760
556.360725	8000.535130	9.736512	-0.107904	4.817772
556.455202	8000.432073	9.741517	-0.107922	4.817741
556.547944	8000.525211	9.746522	-0.107939	4.817768
556.386810	8000.427902	9.751527	-0.107909	4.817740
556.772479	8000.437773	9.756531	-0.107981	4.817741
556.511733	8000.491972	9.761536	-0.107932	4.817758
555.711050	8000.423269	9.766541	-0.107783	4.817742
556.239440	8000.435230	9.771546	-0.107882	4.817743
556.517794	8000.431923	9.776551	-0.107933	4.817741
556.352899	8000.495966	9.781555	-0.107903	4.817760
556.598906	8000.528055	9.786560	-0.107949	4.817769
556.310704	8000.402509	9.791565	-0.107895	4.817733
555.911132	8000.539069	9.796570	-0.107821	4.817775
555.776977	8000.368312	9.801575	-0.107795	4.817725
556.390641	8000.433214	9.806579	-0.107910	4.817742
556.398618	8000.537769	9.811584	-0.107911	4.817773
556.001590	8000.411685	9.816589	-0.107837	4.817737
556.359091	8000.520307	9.821594	-0.107904	4.817768
556.335018	8000.395469	9.826599	-0.107899	4.817731
556.431157	8000.536130	9.831603	-0.107917	4.817772
556.597087	8000.407746	9.836608	-0.107948	4.817733
556.555278	8000.439835	9.841613	-0.107940	4.817743
556.547169	8000.514616	9.846618	-0.107939	4.817765
556.415002	8000.434611	9.851623	-0.107914	4.817742
556.508148	8000.531975	9.856627	-0.107931	4.817770
556.640926	8000.519150	9.861632	-0.107956	4.817766
556.490161	8000.408279	9.866637	-0.107928	4.817734
556.312028	8000.526985	9.871642	-0.107895	4.817770
556.490343	8000.423047	9.876647	-0.107928	4.817738
555.976207	8000.372258	9.881651	-0.107832	4.817725
556.102501	8000.340349	9.886656	-0.107856	4.817715
556.088587	8000.411879	9.891661	-0.107853	4.817737
556.500162	8000.355668	9.896666	-0.107930	4.817718
556.519062	8000.452998	9.901671	-0.107933	4.817747
556.390820	8000.434238	9.906675	-0.107909	4.817742
557.188984	8000.540884	9.911680	-0.108058	4.817770
557.472668	8000.466974	9.916685	-0.108111	4.817747
556.878617	8000.433998	9.921690	-0.108000	4.817740
557.078359	8000.525542	9.926695	-0.108037	4.817766
557.219848	8000.508625	9.931699	-0.108064	4.817760
557.459735	8000.507922	9.936704	-0.108108	4.817759
557.370788	8000.489736	9.941709	-0.108092	4.817754
557.317863	8000.404560	9.946714	-0.108082	4.817729
557.537042	8000.466851	9.951719	-0.108123	4.817747
557.428950	8000.469484	9.956723	-0.108102	4.817748
557.189533	8000.552479	9.961728	-0.108058	4.817773
557.437057	8000.480149	9.966733	-0.108104	4.817751
557.389653	8000.494222	9.971738	-0.108095	4.817755
557.714163	8000.492650	9.976743	-0.108155	4.817753
557.802839	8000.385286	9.981747	-0.108172	4.817721
557.766042	8000.497627	9.986752	-0.108165	4.817755
557.701952	8000.473476	9.991757	-0.108153	4.817748
557.883226	8000.512002	9.996762	-0.108187	4.817758
557.967618	8000.505854	10.001767	-0.108203	4.817756
557.931390	8000.455736	10.006771	-0.108196	4.817742
557.917828	8000.531495	10.011776	-0.108193	4.817764
558.073780	8000.484196	10.016781	-0.108222	4.817749
557.660121	8000.513996	10.021786	-0.108145	4.817760
557.431157	8000.529626	10.026791	-0.108103	4.817766
556.959560	8000.465741	10.031795	-0.108015	4.817749
557.469364	8000.443675	10.036800	-0.108110	4.817740
557.487649	8000.507240	10.041805	-0.108113	4.817759
557.572065	8000.524301	10.046810	-0.108129	4.817763
557.193057	8000.414299	10.051815	-0.108058	4.817733
557.083235	8000.537173	10.056819	-0.108038	4.817769
557.478629	8000.448022	10.061824	-0.108111	4.817741
557.556876	8000.506137	10.066829	-0.108126	4.817758
557.442669	8000.519230	10.071834	-0.108104	4.817763
557.352513	8000.397639	10.076839	-0.108088	4.817727
557.065740	8000.432467	10.081843	-0.108034	4.817739
557.100306	8000.425587	10.086848	-0.108041	4.817736
557.150640	8000.539205	10.091853	-0.108050	4.817770
557.295171	8000.431606	10.096858	-0.108077	4.817737
556.746762	8000.292750	10.101863	-0.107975	4.817699
556.931271	8000.439981	10.106867	-0.108009	4.817741
557.369581	8000.529749	10.111872	-0.108091	4.817766
557.141925	8000.426187	10.116877	-0.108048	4.817736
557.091694	8000.424394	10.121882	-0.108039	4.817736
556.940649	8000.318792	10.126887	-0.108011	4.817705
557.110536	8000.452096	10.131891	-0.108042	4.817744
557.436199	8000.450539	10.136896	-0.108103	4.817742
556.879665	8000.327388	10.141901	-0.107999	4.817708
556.524484	8000.355939	10.146906	-0.107933	4.817718
557.053264	8000.451249	10.151911	-0.108032	4.817744
557.186622	8000.452148	10.156915	-0.108056	4.817744
556.914983	8000.295195	10.161920	-0.108006	4.817699
557.297765	8000.426345	10.166925	-0.108077	4.817736
557.558604	8000.412233	10.171930	-0.108126	4.817730
557.717083	8000.526384	10.176935	-0.108155	4.817763
557.477194	8000.534468	10.181939	-0.108110	4.817767
557.762049	8000.440531	10.186944	-0.108163	4.817738
558.169134	8000.499250	10.191949	-0.108239	4.817753
558.240645	8000.505572	10.196954	-0.108252	4.817755
557.809133	8000.426447	10.201959	-0.108172	4.817734
557.786328	8000.523169	10.206963	-0.108168	4.817762
558.215746	8000.533687	10.211968	-0.108248	4.817763
557.929494	8000.479901	10.216973	-0.108194	4.817749
557.971029	8000.502664	10.221978	-0.108202	4.817755
558.131145	8000.493406	10.226983	-0.108232	4.817752
558.252638	8000.470921	10.231987	-0.108255	4.817745
558.448403	8000.515992	10.236992	-0.108291	4.817757
558.180989	8000.514177	10.241997	-0.108241	4.817758
558.289439	8000.386002	10.247002	-0.108261	4.817719
558.202079	8000.513428	10.252007	-0.108245	4.817758
557.837218	8000.493304	10.257011	-0.108177	4.817753
558.086197	8000.544429	10.262016	-0.108223	4.817767
558.225851	8000.483176	10.267021	-0.108249	4.817748
558.365537	8000.487334	10.272026	-0.108275	4.817749
558.298410	8000.492677	10.277031	-0.108263	4.817751
558.272875	8000.471201	10.282035	-0.108258	4.817745
558.538463	8000.522571	10.287040	-0.108308	4.817759
558.320900	8000.499332	10.292045	-0.108267	4.817753
558.400956	8000.519495	10.297050	-0.108282	4.817758
558.370066	8000.501105	10.302055	-0.108276	4.817753
558.308193	8000.427401	10.307059	-0.108265	4.817732
558.462080	8000.536212	10.312064	-0.108293	4.817763
558.368129	8000.510567	10.317069	-0.108276	4.817756
558.141369	8000.525173	10.322074	-0.108233	4.817761
557.981192	8000.394113	10.327079	-0.108204	4.817723
557.771365	8000.540842	10.332083	-0.108165	4.817768
558.101223	8000.463389	10.337088	-0.108226	4.817743
557.396049	8000.442496	10.342093	-0.108095	4.817740
557.492843	8000.351076	10.347098	-0.108113	4.817713
557.736109	8000.447479	10.352103	-0.108158	4.817740
558.085656	8000.523289	10.357107	-0.108223	4.817761
557.763849	8000.358209	10.362112	-0.108163	4.817714
557.857043	8000.516767	10.367117	-0.108180	4.817760
558.044808	8000.512134	10.372122	-0.108215	4.817758
557.881897	8000.428509	10.377127	-0.108185	4.817734
557.920520	8000.444899	10.382131	-0.108192	4.817739
557.993049	8000.444906	10.387136	-0.108206	4.817738
557.876432	8000.532867	10.392141	-0.108184	4.817765
558.292235	8000.541076	10.397146	-0.108261	4.817765
558.005862	8000.461968	10.402151	-0.108208	4.817743
557.972505	8000.444598	10.407155	-0.108202	4.817738
557.954127	8000.444326	10.412160	-0.108198	4.817738
557.820762	8000.437094	10.417165	-0.108173	4.817737
558.086386	8000.538047	10.422170	-0.108223	4.817765
557.668278	8000.356786	10.427175	-0.108145	4.817714
557.787517	8000.544209	10.432179	-0.108167	4.817768
557.692995	8000.367695	10.437184	-0.108149	4.817717
557.828579	8000.436145	10.442189	-0.108175	4.817736
557.855982	8000.454480	10.447194	-0.108180	4.817742
557.828617	8000.357019	10.452199	-0.108175	4.817713
557.968679	8000.448744	10.457203	-0.108201	4.817739
558.164419	8000.530738	10.462208	-0.108237	4.817763
558.463616	8000.530906	10.467213	-0.108293	4.817762
558.381926	8000.520211	10.472218	-0.108278	4.817759
558.613194	8000.526768	10.477223	-0.108321	4.817760
558.630530	8000.397255	10.482227	-0.108324	4.817721
558.791582	8000.539932	10.487232	-0.108354	4.817763
558.705693	8000.516515	10.492237	-0.108338	4.817756
558.879772	8000.514848	10.497242	-0.108370	4.817755
558.665481	8000.439961	10.502247	-0.108330	4.817734
558.273894	8000.451094	10.507251	-0.108257	4.817739
558.322659	8000.459193	10.512256	-0.108266	4.817741
558.648111	8000.517771	10.517261	-0.108327	4.817757
557.874691	8000.369275	10.522266	-0.108183	4.817716
558.270798	8000.465812	10.527271	-0.108257	4.817743
557.941666	8000.447267	10.532275	-0.108195	4.817739
558.045646	8000.353842	10.537280	-0.108215	4.817711
558.426841	8000.339387	10.542285	-0.108286	4.817705
558.449811	8000.456826	10.547290	-0.108290	4.817740
558.494370	8000.558759	10.552295	-0.108298	4.817770
558.255140	8000.408602	10.557299	-0.108254	4.817726
558.522484	8000.557058	10.562304	-0.108303	4.817769
558.529791	8000.493863	10.567309	-0.108305	4.817750
558.431592	8000.454441	10.572314	-0.108286	4.817739
558.349802	8000.547134	10.577319	-0.108271	4.817767
558.224466	8000.401814	10.582323	-0.108248	4.817724
558.187721	8000.439253	10.587328	-0.108241	4.817736
558.151347	8000.460872	10.592333	-0.108234	4.817742
558.317058	8000.544537	10.597338	-0.108265	4.817766
558.475776	8000.410769	10.602343	-0.108294	4.817726
558.414977	8000.404600	10.607347	-0.108283	4.817724
558.642980	8000.550369	10.612352	-0.108326	4.817767
558.483991	8000.394004	10.617357	-0.108296	4.817721
558.868829	8000.551570	10.622362	-0.108368	4.817766
558.749229	8000.548758	10.627367	-0.108345	4.817766
558.696560	8000.405557	10.632371	-0.108335	4.817724
559.018898	8000.545327	10.637376	-0.108396	4.817763
558.395349	8000.437005	10.642381	-0.108279	4.817734
558.565410	8000.445828	10.647386	-0.108311	4.817736
558.685751	8000.423327	10.652391	-0.108333	4.817729
558.420122	8000.435253	10.657395	-0.108284	4.817734
558.656225	8000.437660	10.662400	-0.108328	4.817733
558.373429	8000.429290	10.667405	-0.108275	4.817732
558.382421	8000.333416	10.672410	-0.108277	4.817704
558.335997	8000.336953	10.677415	-0.108268	4.817705
558.385267	8000.500143	10.682419	-0.108277	4.817753
558.960812	8000.512807	10.687424	-0.108384	4.817754
559.011453	8000.403827	10.692429	-0.108394	4.817722
558.798984	8000.527309	10.697434	-0.108354	4.817759
558.849332	8000.472130	10.702439	-0.108364	4.817743
558.940251	8000.457638	10.707443	-0.108381	4.817738
558.790500	8000.431173	10.712448	-0.108353	4.817731
558.740309	8000.538046	10.717453	-0.108343	4.817763
558.792306	8000.445967	10.722458	-0.108353	4.817735
558.888768	8000.539166	10.727463	-0.108371	4.817762
558.586339	8000.436611	10.732467	-0.108314	4.817733
558.829339	8000.444395	10.737472	-0.108360	4.817734
558.813210	8000.534887	10.742477	-0.108357	4.817761
558.714895	8000.558763	10.747482	-0.108338	4.817769
558.867541	8000.318350	10.752487	-0.108367	4.817697
558.880996	8000.564362	10.757491	-0.108369	4.817770
559.044947	8000.462320	10.762496	-0.108400	4.817739
558.707695	8000.458425	10.767501	-0.108337	4.817739
559.133359	8000.538521	10.772506	-0.108416	4.817761
558.857508	8000.342459	10.777511	-0.108365	4.817704
558.862172	8000.525042	10.782515	-0.108366	4.817758
558.798078	8000.472404	10.787520	-0.108354	4.817743
558.797780	8000.425978	10.792525	-0.108354	4.817729
558.441379	8000.443957	10.797530	-0.108287	4.817736
558.232603	8000.320624	10.802535	-0.108248	4.817700
557.884945	8000.355613	10.807539	-0.108184	4.817712
558.438568	8000.314147	10.812544	-0.108287	4.817698
558.776553	8000.444648	10.817549	-0.108350	4.817735
558.671844	8000.349215	10.822554	-0.108330	4.817707
558.193235	8000.312653	10.827559	-0.108241	4.817698
558.464836	8000.352505	10.832563	-0.108291	4.817709
558.577633	8000.419567	10.837568	-0.108312	4.817728
558.525476	8000.429351	10.842573	-0.108303	4.817731
558.687921	8000.458107	10.847578	-0.108333	4.817739
558.663046	8000.457741	10.852583	-0.108328	4.817739
558.862032	8000.555610	10.857587	-0.108365	4.817767
558.869138	8000.370031	10.862592	-0.108367	4.817712
558.701812	8000.469909	10.867597	-0.108335	4.817743
559.008817	8000.514503	10.872602	-0.108393	4.817754
559.324897	8000.556066	10.877607	-0.108451	4.817765
559.268307	8000.529913	10.882611	-0.108441	4.817758
559.443275	8000.469178	10.887616	-0.108473	4.817739
559.403133	8000.533999	10.892621	-0.108466	4.817758
558.984689	8000.448730	10.897626	-0.108388	4.817735
559.016819	8000.449199	10.902631	-0.108394	4.817735
558.873081	8000.546259	10.907635	-0.108367	4.817764
559.109718	8000.530740	10.912640	-0.108411	4.817759
558.675127	8000.403035	10.917645	-0.108330	4.817723
558.821235	8000.548659	10.922650	-0.108357	4.817765
558.940909	8000.432252	10.927655	-0.108380	4.817730
558.888973	8000.528549	10.932659	-0.108370	4.817759
559.054928	8000.452912	10.937664	-0.108401	4.817736
559.180344	8000.522272	10.942669	-0.108424	4.817756
559.048129	8000.530880	10.947674	-0.108400	4.817759
559.140395	8000.445721	10.952679	-0.108417	4.817734
559.195129	8000.544639	10.957683	-0.108427	4.817763
559.286052	8000.454185	10.962688	-0.108444	4.817735
559.156279	8000.513470	10.967693	-0.108420	4.817753
559.349959	8000.540576	10.972698	-0.108456	4.817761
558.684311	8000.424250	10.977703	-0.108332	4.817729
558.737926	8000.438750	10.982707	-0.108342	4.817733
559.128869	8000.453980	10.987712	-0.108414	4.817736
559.031484	8000.466264	10.992717	-0.108396	4.817740
558.708501	8000.442533	10.997722	-0.108336	4.817734
558.780008	8000.360235	11.002727	-0.108349	4.817710
558.752207	8000.462161	11.007731	-0.108344	4.817740
558.863678	8000.354074	11.012736	-0.108365	4.817708
559.045606	8000.520268	11.017741	-0.108399	4.817756
558.993696	8000.534275	11.022746	-0.108389	4.817760
559.116011	8000.546619	11.027751	-0.108412	4.817763
558.958424	8000.438803	11.032755	-0.108382	4.817732
559.512124	8000.435322	11.037760	-0.108486	4.817729
559.596924	8000.522022	11.042765	-0.108501	4.817754
559.556941	8000.541479	11.047770	-0.108494	4.817760
559.413432	8000.558361	11.052775	-0.108467	4.817766
559.313000	8000.543170	11.057779	-0.108448	4.817762
559.324425	8000.426228	11.062784	-0.108450	4.817727
559.400592	8000.524407	11.067789	-0.108465	4.817756
559.356622	8000.515319	11.072794	-0.108457	4.817753
559.571940	8000.527974	11.077799	-0.108497	4.817756
559.564046	8000.496205	11.082803	-0.108495	4.817747
559.571885	8000.535355	11.087808	-0.108497	4.817758
559.793634	8000.506957	11.092813	-0.108538	4.817749
559.595892	8000.494557	11.097818	-0.108501	4.817746
559.490122	8000.537314	11.102823	-0.108481	4.817759
559.572886	8000.532197	11.107827	-0.108497	4.817757
559.531233	8000.445072	11.112832	-0.108489	4.817732
559.270268	8000.546742	11.117837	-0.108440	4.817763
559.371679	8000.513413	11.122842	-0.108459	4.817753
559.602488	8000.546340	11.127847	-0.108502	4.817761
559.559037	8000.508775	11.132851	-0.108494	4.817750
559.230619	8000.451202	11.137856	-0.108433	4.817735
559.726765	8000.558710	11.142861	-0.108525	4.817764
559.472713	8000.526493	11.147866	-0.108478	4.817756
559.363646	8000.553376	11.152871	-0.108457	4.817764
559.216815	8000.366591	11.157875	-0.108430	4.817710
559.239541	8000.553661	11.162880	-0.108434	4.817765
559.072100	8000.446755	11.167885	-0.108403	4.817734
559.636759	8000.470866	11.172890	-0.108508	4.817739
559.635471	8000.527817	11.177895	-0.108508	4.817756
559.459770	8000.490420	11.182899	-0.108475	4.817745
559.268674	8000.555135	11.187904	-0.108440	4.817765
559.481534	8000.416885	11.192909	-0.108479	4.817724
559.662014	8000.532420	11.197914	-0.108513	4.817757
559.815810	8000.532566	11.202919	-0.108541	4.817756
559.631368	8000.522471	11.207923	-0.108507	4.817754
559.643938	8000.557470	11.212928	-0.108509	4.817764
559.324316	8000.321727	11.217933	-0.108450	4.817696
559.535538	8000.531610	11.222938	-0.108489	4.817757
559.232893	8000.460699	11.227943	-0.108433	4.817738
559.621069	8000.547632	11.232947	-0.108505	4.817762
559.314711	8000.459787	11.237952	-0.108448	4.817737
558.820210	8000.233088	11.242957	-0.108356	4.817672
559.115683	8000.473743	11.247962	-0.108411	4.817742
559.191308	8000.352469	11.252967	-0.108425	4.817706
559.109560	8000.448329	11.257971	-0.108410	4.817734
559.224033	8000.425742	11.262976	-0.108431	4.817727
559.420470	8000.443393	11.267981	-0.108467	4.817732
559.234429	8000.560933	11.272986	-0.108433	4.817767
559.498149	8000.427650	11.277991	-0.108482	4.817727
559.603308	8000.520979	11.282995	-0.108502	4.817754
559.451833	8000.343620	11.288000	-0.108473	4.817702
559.541785	8000.470486	11.293005	-0.108490	4.817739
559.472826	8000.520113	11.298010	-0.108477	4.817754
559.433667	8000.454125	11.303015	-0.108470	4.817735
559.317077	8000.549474	11.308019	-0.108448	4.817763
559.537255	8000.460917	11.313024	-0.108489	4.817736
559.325359	8000.540097	11.318029	-0.108450	4.817761
559.247573	8000.447167	11.323034	-0.108435	4.817734
559.261933	8000.449486	11.328039	-0.108438	4.817734
559.127106	8000.545622	11.333043	-0.108413	4.817763
559.441934	8000.540747	11.338048	-0.108471	4.817760
559.743940	8000.441785	11.343053	-0.108527	4.817730
559.502479	8000.509981	11.348058	-0.108482	4.817751
559.423976	8000.457131	11.353063	-0.108468	4.817736
559.595099	8000.536658	11.358067	-0.108500	4.817758
559.690042	8000.554931	11.363072	-0.108517	4.817763
559.713884	8000.542619	11.368077	-0.108522	4.817760
559.455027	8000.416434	11.373082	-0.108473	4.817724
559.395154	8000.459864	11.378087	-0.108462	4.817737
559.636084	8000.535141	11.383091	-0.108507	4.817758
559.582355	8000.544901	11.388096	-0.108497	4.817761
559.534175	8000.526256	11.393101	-0.108488	4.817756
559.286393	8000.439271	11.398106	-0.108442	4.817731
559.323273	8000.474626	11.403111	-0.108449	4.817741
559.410337	8000.543424	11.408115	-0.108465	4.817761
559.301403	8000.457421	11.413120	-0.108445	4.817736
559.615076	8000.483124	11.418125	-0.108503	4.817743
559.359603	8000.482538	11.423130	-0.108456	4.817743
559.434049	8000.578581	11.428135	-0.108469	4.817772
559.794842	8000.420346	11.433139	-0.108536	4.817723
559.571545	8000.538395	11.438144	-0.108495	4.817759
559.518988	8000.557667	11.443149	-0.108485	4.817765
559.926733	8000.487689	11.448154	-0.108561	4.817743
559.853884	8000.496113	11.453159	-0.108547	4.817745
559.680993	8000.509399	11.458163	-0.108515	4.817750
559.731479	8000.519634	11.463168	-0.108525	4.817753
559.498199	8000.436025	11.468173	-0.108481	4.817729
559.529101	8000.428037	11.473178	-0.108487	4.817727
559.737667	8000.528160	11.478183	-0.108526	4.817755
559.575665	8000.499404	11.483187	-0.108495	4.817748
559.800447	8000.517473	11.488192	-0.108537	4.817752
559.535463	8000.539956	11.493197	-0.108488	4.817760
559.733358	8000.515429	11.498202	-0.108525	4.817752
559.751443	8000.471382	11.503207	-0.108528	4.817739
559.789061	8000.505693	11.508211	-0.108535	4.817748
559.851482	8000.534039	11.513216	-0.108547	4.817757
559.882283	8000.539765	11.518221	-0.108552	4.817758
559.544967	8000.524260	11.523226	-0.108490	4.817755
559.790003	8000.444508	11.528231	-0.108535	4.817730
560.029376	8000.515543	11.533235	-0.108580	4.817750
560.006808	8000.484614	11.538240	-0.108576	4.817741
560.010744	8000.531092	11.543245	-0.108576	4.817755
560.354909	8000.438025	11.548250	-0.108640	4.817726
560.379661	8000.495359	11.553255	-0.108645	4.817743
560.237303	8000.497487	11.558259	-0.108618	4.817744
560.272357	8000.455798	11.563264	-0.108625	4.817732
560.181416	8000.513543	11.568269	-0.108608	4.817749
560.164655	8000.455268	11.573274	-0.108605	4.817732
560.090056	8000.499538	11.578279	-0.108591	4.817745
560.260415	8000.497818	11.583283	-0.108623	4.817744
560.140719	8000.507664	11.588288	-0.108600	4.817748
559.960254	8000.558819	11.593293	-0.108567	4.817763
559.823907	8000.385900	11.598298	-0.108541	4.817713
560.263579	8000.550610	11.603303	-0.108623	4.817760
559.823162	8000.530425	11.608307	-0.108541	4.817756
559.977003	8000.547453	11.613312	-0.108570	4.817760
559.975612	8000.544266	11.618317	-0.108569	4.817759
559.874662	8000.422508	11.623322	-0.108551	4.817724
559.983617	8000.524334	11.628327	-0.108571	4.817753
559.807780	8000.525971	11.633331	-0.108538	4.817754
559.932014	8000.543619	11.638336	-0.108561	4.817759
559.774366	8000.408368	11.643341	-0.108532	4.817720
559.827672	8000.526258	11.648346	-0.108542	4.817754
559.915403	8000.449471	11.653351	-0.108558	4.817731
559.767100	8000.563346	11.658355	-0.108530	4.817766
559.772467	8000.470580	11.663360	-0.108531	4.817738
559.970377	8000.456604	11.668365	-0.108568	4.817733
559.953761	8000.521770	11.673370	-0.108565	4.817753
559.976397	8000.554807	11.678375	-0.108569	4.817762
560.113934	8000.439715	11.683379	-0.108595	4.817728
560.199970	8000.547536	11.688384	-0.108611	4.817759
560.044098	8000.458732	11.693389	-0.108582	4.817734
560.031116	8000.533448	11.698394	-0.108579	4.817756
560.296990	8000.547901	11.703399	-0.108629	4.817759
560.015078	8000.541649	11.708403	-0.108576	4.817758
560.098358	8000.463742	11.713408	-0.108592	4.817735
560.181254	8000.555692	11.718413	-0.108607	4.817762
559.992050	8000.499104	11.723418	-0.108572	4.817746
560.038110	8000.456522	11.728423	-0.108581	4.817733
559.651642	8000.546855	11.733427	-0.108509	4.817761
559.888783	8000.492308	11.738432	-0.108553	4.817744
559.740365	8000.459532	11.743437	-0.108525	4.817735
559.689018	8000.522078	11.748442	-0.108515	4.817754
560.184582	8000.571554	11.753447	-0.108608	4.817766
560.146568	8000.522462	11.758451	-0.108601	4.817752
559.752316	8000.456535	11.763456	-0.108527	4.817734
559.700500	8000.384031	11.768461	-0.108517	4.817713
559.531004	8000.355166	11.773466	-0.108486	4.817705
559.334796	8000.338570	11.778471	-0.108449	4.817701
559.152357	8000.340111	11.783475	-0.108415	4.817702
559.154508	8000.372846	11.788480	-0.108416	4.817712
559.130913	8000.380938	11.793485	-0.108411	4.817714
558.914020	8000.285969	11.798490	-0.108371	4.817687
559.412331	8000.254243	11.803495	-0.108464	4.817676
559.489488	8000.548669	11.808499	-0.108478	4.817763
559.669627	8000.402553	11.813504	-0.108511	4.817719
559.542960	8000.457663	11.818509	-0.108488	4.817735
559.591379	8000.519564	11.823514	-0.108497	4.817753
559.810387	8000.525942	11.828519	-0.108538	4.817754
559.624324	8000.514769	11.833523	-0.108503	4.817752
560.165579	8000.488953	11.838528	-0.108604	4.817742
560.167387	8000.469987	11.843533	-0.108604	4.817736
560.115288	8000.448119	11.848538	-0.108594	4.817730
560.111319	8000.552508	11.853543	-0.108594	4.817761
559.857271	8000.444328	11.858547	-0.108546	4.817730
559.821874	8000.575686	11.863552	-0.108540	4.817769
560.381474	8000.533259	11.868557	-0.108644	4.817754
560.342505	8000.532685	11.873562	-0.108637	4.817754
560.243741	8000.429949	11.878567	-0.108618	4.817724
559.851087	8000.506475	11.883571	-0.108545	4.817748
560.292211	8000.510841	11.888576	-0.108627	4.817748
559.917955	8000.540160	11.893581	-0.108557	4.817758
559.682923	8000.448085	11.898586	-0.108514	4.817732
559.819239	8000.472240	11.903591	-0.108539	4.817739
560.063810	8000.525416	11.908595	-0.108585	4.817753
559.850457	8000.422053	11.913600	-0.108545	4.817724
559.693989	8000.473561	11.918605	-0.108516	4.817739
559.960756	8000.532338	11.923610	-0.108565	4.817756
560.196530	8000.464055	11.928615	-0.108609	4.817734
560.119412	8000.569480	11.933619	-0.108595	4.817766
560.209570	8000.457913	11.938624	-0.108612	4.817733
560.239225	8000.461512	11.943629	-0.108617	4.817734
560.164931	8000.538492	11.948634	-0.108603	4.817757
560.185299	8000.560946	11.953639	-0.108607	4.817763
560.091203	8000.546902	11.958643	-0.108589	4.817759
559.683801	8000.330968	11.963648	-0.108513	4.817697
560.019410	8000.481487	11.968653	-0.108576	4.817740
559.873953	8000.470909	11.973658	-0.108549	4.817738
559.651668	8000.449709	11.978663	-0.108507	4.817733
559.960534	8000.441581	11.983667	-0.108565	4.817729
560.198489	8000.513650	11.988672	-0.108609	4.817749
559.910661	8000.535798	11.993677	-0.108556	4.817757
559.627899	8000.547471	11.998682	-0.108503	4.817762
560.189346	8000.471309	12.003687	-0.108607	4.817737
560.225729	8000.528814	12.008691	-0.108614	4.817753
560.109751	8000.509174	12.013696	-0.108593	4.817748
560.110528	8000.545055	12.018701	-0.108593	4.817759
559.926461	8000.457947	12.023706	-0.108558	4.817734
560.074856	8000.548748	12.028711	-0.108586	4.817760
560.229002	8000.508808	12.033715	-0.108615	4.817748
560.216734	8000.499131	12.038720	-0.108612	4.817745
560.252851	8000.542916	12.043725	-0.108619	4.817758
559.918728	8000.543283	12.048730	-0.108557	4.817759
560.099786	8000.448876	12.053735	-0.108591	4.817730
560.226461	8000.547799	12.058739	-0.108614	4.817759
559.926790	8000.450553	12.063744	-0.108558	4.817732
560.103118	8000.435205	12.068749	-0.108591	4.817726
559.974659	8000.568362	12.073754	-0.108567	4.817766
560.096529	8000.453040	12.078759	-0.108590	4.817732
560.041527	8000.437461	12.083763	-0.108580	4.817727
559.945708	8000.541556	12.088768	-0.108562	4.817758
560.348256	8000.564346	12.093773	-0.108637	4.817763
560.300920	8000.514062	12.098778	-0.108628	4.817749
560.225209	8000.471802	12.103783	-0.108614	4.817737
560.380054	8000.516276	12.108787	-0.108643	4.817749
560.210943	8000.527506	12.113792	-0.108611	4.817753
560.302299	8000.447607	12.118797	-0.108628	4.817729
559.873972	8000.521500	12.123802	-0.108548	4.817753
559.945311	8000.457133	12.128807	-0.108561	4.817734
560.124791	8000.544170	12.133811	-0.108595	4.817758
559.981879	8000.450281	12.138816	-0.108568	4.817731
559.938757	8000.468637	12.143821	-0.108560	4.817737
559.858671	8000.433699	12.148826	-0.108545	4.817727
559.849427	8000.563331	12.153831	-0.108544	4.817765
560.185294	8000.550325	12.158835	-0.108606	4.817760
560.046000	8000.440664	12.163840	-0.108580	4.817728
559.904954	8000.472353	12.168845	-0.108554	4.817738
559.898429	8000.423724	12.173850	-0.108553	4.817724
560.023520	8000.571154	12.178855	-0.108576	4.817767
560.148092	8000.522339	12.183859	-0.108599	4.817752
559.747828	8000.422563	12.188864	-0.108524	4.817724
559.856739	8000.537048	12.193869	-0.108545	4.817758
559.670414	8000.421423	12.198874	-0.108510	4.817724
559.527523	8000.396114	12.203879	-0.108483	4.817717
559.756922	8000.442735	12.208883	-0.108526	4.817730
559.328976	8000.437507	12.213888	-0.108446	4.817730
559.796898	8000.330431	12.218893	-0.108533	4.817697
559.489028	8000.330131	12.223898	-0.108476	4.817698
559.718536	8000.480146	12.228903	-0.108519	4.817741
559.646142	8000.463256	12.233907	-0.108505	4.817737
559.803440	8000.450793	12.238912	-0.108535	4.817732
560.135094	8000.369147	12.243917	-0.108596	4.817707
559.808981	8000.551099	12.248922	-0.108536	4.817762
559.511480	8000.447557	12.253927	-0.108480	4.817733
559.823549	8000.347688	12.258931	-0.108538	4.817702
559.698089	8000.447128	12.263936	-0.108515	4.817732
559.634275	8000.464125	12.268941	-0.108503	4.817737
559.564856	8000.360767	12.273946	-0.108490	4.817707
559.793289	8000.338797	12.278951	-0.108532	4.817699
559.606483	8000.345549	12.283955	-0.108498	4.817702
559.491303	8000.337527	12.288960	-0.108476	4.817700
559.750353	8000.460545	12.293965	-0.108524	4.817735
559.462559	8000.427833	12.298970	-0.108471	4.817727
559.922974	8000.399774	12.303975	-0.108557	4.817717
559.825548	8000.333985	12.308979	-0.108538	4.817698
559.642373	8000.351341	12.313984	-0.108504	4.817704
560.180476	8000.462631	12.318989	-0.108604	4.817734
559.968262	8000.542862	12.323994	-0.108565	4.817759
560.274122	8000.345838	12.328999	-0.108622	4.817699
559.859440	8000.443142	12.334003	-0.108545	4.817730
560.004183	8000.529668	12.339008	-0.108572	4.817755
559.764081	8000.449124	12.344013	-0.108527	4.817732
559.974947	8000.431117	12.349018	-0.108566	4.817726
560.095530	8000.459262	12.354023	-0.108588	4.817734
559.907189	8000.455440	12.359027	-0.108553	4.817733
559.871139	8000.459129	12.364032	-0.108547	4.817734
559.876479	8000.358978	12.369037	-0.108548	4.817705
559.757234	8000.419472	12.374042	-0.108525	4.817723
560.008316	8000.468523	12.379047	-0.108572	4.817737
560.253642	8000.440472	12.384051	-0.108618	4.817727
560.190977	8000.548220	12.389056	-0.108606	4.817759
560.368661	8000.549772	12.394061	-0.108639	4.817759
560.322595	8000.450975	12.399066	-0.108631	4.817730
560.334453	8000.569312	12.404071	-0.108633	4.817765
560.162431	8000.439124	12.409075	-0.108601	4.817727
560.256481	8000.562889	12.414080	-0.108618	4.817763
560.630674	8000.468152	12.419085	-0.108688	4.817734
560.097473	8000.460321	12.424090	-0.108589	4.817734
560.287100	8000.507416	12.429095	-0.108624	4.817747
560.197303	8000.537747	12.434099	-0.108607	4.817756
559.994340	8000.445087	12.439104	-0.108569	4.817730
559.585687	8000.466517	12.444109	-0.108493	4.817738
559.601850	8000.358085	12.449114	-0.108496	4.817706
559.510701	8000.460138	12.454119	-0.108479	4.817736
559.617236	8000.444819	12.459123	-0.108499	4.817731
560.027081	8000.448724	12.464128	-0.108575	4.817731
560.215073	8000.573867	12.469133	-0.108610	4.817767
560.009709	8000.433695	12.474138	-0.108572	4.817726
560.170632	8000.553165	12.479143	-0.108602	4.817761
559.960581	8000.449851	12.484147	-0.108563	4.817731
559.538817	8000.444713	12.489152	-0.108484	4.817732
559.816891	8000.371776	12.494157	-0.108536	4.817709
560.214360	8000.543250	12.499162	-0.108610	4.817758
560.102987	8000.465650	12.504167	-0.108589	4.817735
560.194766	8000.459611	12.509171	-0.108606	4.817733
560.090682	8000.454916	12.514176	-0.108587	4.817732
560.211177	8000.373335	12.519181	-0.108609	4.817708
559.982248	8000.573595	12.524186	-0.108567	4.817768
559.685920	8000.344521	12.529191	-0.108511	4.817701
559.963081	8000.352807	12.534195	-0.108563	4.817703
559.422457	8000.474639	12.539200	-0.108462	4.817741
559.990773	8000.366926	12.544205	-0.108568	4.817707
560.092816	8000.467595	12.549210	-0.108587	4.817736
560.245986	8000.466677	12.554215	-0.108616	4.817735
560.056782	8000.559906	12.559219	-0.108580	4.817763
560.048951	8000.435295	12.564224	-0.108579	4.817727
560.376265	8000.545604	12.569229	-0.108640	4.817758
560.246698	8000.516268	12.574234	-0.108616	4.817750
559.950685	8000.451783	12.579239	-0.108561	4.817732
560.272987	8000.467064	12.584243	-0.108621	4.817735
560.083988	8000.546580	12.589248	-0.108585	4.817759
559.964252	8000.447757	12.594253	-0.108563	4.817731
560.078955	8000.449439	12.599258	-0.108584	4.817731
559.922006	8000.308925	12.604263	-0.108555	4.817690
560.054535	8000.352014	12.609267	-0.108580	4.817702
560.211193	8000.567430	12.614272	-0.108609	4.817765
560.099883	8000.351621	12.619277	-0.108588	4.817702
560.049162	8000.340325	12.624282	-0.108579	4.817699
560.025117	8000.477124	12.629287	-0.108574	4.817739
559.896048	8000.380275	12.634291	-0.108550	4.817711
559.751236	8000.469935	12.639296	-0.108523	4.817738
560.004480	8000.350212	12.644301	-0.108570	4.817702
559.949427	8000.364173	12.649306	-0.108560	4.817706
560.214420	8000.570629	12.654311	-0.108609	4.817766
560.535253	8000.541578	12.659315	-0.108669	4.817756
560.351713	8000.438651	12.664320	-0.108635	4.817726
560.410193	8000.455334	12.669325	-0.108646	4.817731
559.936667	8000.433609	12.674330	-0.108558	4.817727
560.367752	8000.462092	12.679335	-0.108638	4.817733
560.184697	8000.415091	12.684339	-0.108604	4.817720
560.111511	8000.354933	12.689344	-0.108590	4.817703
560.026417	8000.358958	12.694349	-0.108574	4.817704
559.555470	8000.348879	12.699354	-0.108486	4.817703
559.904561	8000.360331	12.704359	-0.108551	4.817705
560.018053	8000.333509	12.709363	-0.108572	4.817697
560.305659	8000.426352	12.714368	-0.108626	4.817723
560.208680	8000.457633	12.719373	-0.108608	4.817733
560.452122	8000.534004	12.724378	-0.108653	4.817754
560.359410	8000.438742	12.729383	-0.108636	4.817726
560.389898	8000.474004	12.734387	-0.108642	4.817737
560.363069	8000.552737	12.739392	-0.108637	4.817760
559.994665	8000.467143	12.744397	-0.108568	4.817736
560.370922	8000.546519	12.749402	-0.108638	4.817758
560.514701	8000.444179	12.754407	-0.108665	4.817727
560.415081	8000.571430	12.759411	-0.108646	4.817765
560.423196	8000.441777	12.764416	-0.108648	4.817727
560.485926	8000.576687	12.769421	-0.108659	4.817767
560.533061	8000.451827	12.774426	-0.108668	4.817729
560.325219	8000.540562	12.779431	-0.108629	4.817757
560.797076	8000.551711	12.784435	-0.108717	4.817758
560.279058	8000.412221	12.789440	-0.108621	4.817719
559.992886	8000.470265	12.794445	-0.108567	4.817737
559.858872	8000.438755	12.799450	-0.108542	4.817729
560.449336	8000.560312	12.804455	-0.108652	4.817762
559.988967	8000.342543	12.809459	-0.108567	4.817699
559.665604	8000.352566	12.814464	-0.108506	4.817704
559.800826	8000.359824	12.819469	-0.108532	4.817705
559.481462	8000.260184	12.824474	-0.108472	4.817677
559.597448	8000.269269	12.829479	-0.108494	4.817679
560.480494	8000.465805	12.834483	-0.108658	4.817734
560.222156	8000.475725	12.839488	-0.108610	4.817738
560.187324	8000.370764	12.844493	-0.108603	4.817707
559.950903	8000.331420	12.849498	-0.108559	4.817696
559.758373	8000.311713	12.854503	-0.108523	4.817691
559.954164	8000.349400	12.859507	-0.108560	4.817702
559.734516	8000.472778	12.864512	-0.108519	4.817739
560.020914	8000.252259	12.869517	-0.108572	4.817673
559.993113	8000.354187	12.874522	-0.108567	4.817703
559.765923	8000.371951	12.879527	-0.108525	4.817709
560.238884	8000.367287	12.884531	-0.108613	4.817706
559.969936	8000.534252	12.889536	-0.108563	4.817756
559.708481	8000.341562	12.894541	-0.108514	4.817700
559.753272	8000.362263	12.899546	-0.108522	4.817706
560.303532	8000.428366	12.904551	-0.108625	4.817724
560.156040	8000.430419	12.909555	-0.108597	4.817725
560.087506	8000.373494	12.914560	-0.108585	4.817708
560.239368	8000.387327	12.919565	-0.108613	4.817712
560.053634	8000.432076	12.924570	-0.108578	4.817726
560.227914	8000.477889	12.929575	-0.108611	4.817739
560.327124	8000.444528	12.934579	-0.108629	4.817728
560.259386	8000.354908	12.939584	-0.108616	4.817702
560.394266	8000.475052	12.944589	-0.108642	4.817737
560.559319	8000.567153	12.949594	-0.108672	4.817763
560.037763	8000.465593	12.954599	-0.108575	4.817736
560.328134	8000.457195	12.959603	-0.108629	4.817732
560.063171	8000.443807	12.964608	-0.108580	4.817729
560.097341	8000.474903	12.969613	-0.108586	4.817738
560.170786	8000.392632	12.974618	-0.108600	4.817714
560.410432	8000.520644	12.979623	-0.108644	4.817750
560.299071	8000.484190	12.984627	-0.108624	4.817740
560.439802	8000.414512	12.989632	-0.108650	4.817719
560.204571	8000.469084	12.994637	-0.108606	4.817736
560.295396	8000.451425	12.999642	-0.108623	4.817730
560.351615	8000.530322	13.004647	-0.108633	4.817753
560.162159	8000.201533	13.009651	-0.108598	4.817657
560.435313	8000.561089	13.014656	-0.108649	4.817762
560.320309	8000.323069	13.019661	-0.108627	4.817692
559.902864	8000.236759	13.024666	-0.108550	4.817669
560.322441	8000.439151	13.029671	-0.108628	4.817727
559.872161	8000.288000	13.034675	-0.108544	4.817684
560.285436	8000.344706	13.039680	-0.108621	4.817699
560.067787	8000.376326	13.044685	-0.108580	4.817709
560.393610	8000.448630	13.049690	-0.108641	4.817729
559.929167	8000.346857	13.054695	-0.108554	4.817701
560.185530	8000.474057	13.059699	-0.108602	4.817738
560.500293	8000.442806	13.064704	-0.108661	4.817727
560.204165	8000.485933	13.069709	-0.108606	4.817741
560.235598	8000.400935	13.074714	-0.108611	4.817716
560.345907	8000.504892	13.079719	-0.108632	4.817746
560.438422	8000.468267	13.084723	-0.108649	4.817735
560.369281	8000.375461	13.089728	-0.108636	4.817708
560.496801	8000.457515	13.094733	-0.108660	4.817731
560.368849	8000.550589	13.099738	-0.108636	4.817759
560.322813	8000.458122	13.104743	-0.108628	4.817732
560.765524	8000.458291	13.109747	-0.108710	4.817730
560.241162	8000.454810	13.114752	-0.108612	4.817732
560.571776	8000.460718	13.119757	-0.108674	4.817732
560.430252	8000.434372	13.124762	-0.108647	4.817725
560.770752	8000.564922	13.129767	-0.108711	4.817762
560.482517	8000.373943	13.134771	-0.108657	4.817707
560.688321	8000.544717	13.139776	-0.108696	4.817756
560.595498	8000.466333	13.144781	-0.108678	4.817734
560.530325	8000.557163	13.149786	-0.108666	4.817761
560.832452	8000.558434	13.154791	-0.108722	4.817760
561.018293	8000.474647	13.159795	-0.108757	4.817734
560.829921	8000.449722	13.164800	-0.108722	4.817728
560.779270	8000.403610	13.169805	-0.108712	4.817714
561.006799	8000.565209	13.174810	-0.108755	4.817761
560.991926	8000.461592	13.179815	-0.108752	4.817730
560.802511	8000.465139	13.184819	-0.108717	4.817732
560.751176	8000.524521	13.189824	-0.108707	4.817750
560.867473	8000.534668	13.194829	-0.108729	4.817753
560.645024	8000.545115	13.199834	-0.108687	4.817757
560.903392	8000.503541	13.204839	-0.108735	4.817743
560.912908	8000.467807	13.209843	-0.108737	4.817733
560.609700	8000.527710	13.214848	-0.108681	4.817752
561.043924	8000.557298	13.219853	-0.108761	4.817758
560.823629	8000.446444	13.224858	-0.108720	4.817727
560.777344	8000.455258	13.229863	-0.108712	4.817729
560.814920	8000.561314	13.234867	-0.108719	4.817761
560.797034	8000.450269	13.239872	-0.108715	4.817728
560.824894	8000.472832	13.244877	-0.108720	4.817734
561.029250	8000.563403	13.249882	-0.108759	4.817760
560.625191	8000.455125	13.254887	-0.108683	4.817730
561.026615	8000.544369	13.259891	-0.108758	4.817755
560.678592	8000.519209	13.264896	-0.108693	4.817749
560.982266	8000.572201	13.269901	-0.108750	4.817763
561.085224	8000.486142	13.274906	-0.108769	4.817737
561.069337	8000.462695	13.279911	-0.108766	4.817730
561.123301	8000.482477	13.284915	-0.108776	4.817736
560.829442	8000.550958	13.289920	-0.108721	4.817758
560.894772	8000.436915	13.294925	-0.108733	4.817724
561.092236	8000.550595	13.299930	-0.108770	4.817756
560.962119	8000.453726	13.304935	-0.108746	4.817728
560.962156	8000.581388	13.309939	-0.108746	4.817766
560.889005	8000.556045	13.314944	-0.108732	4.817759
560.883164	8000.476828	13.319949	-0.108731	4.817735
560.832689	8000.365304	13.324954	-0.108721	4.817703
560.992766	8000.472104	13.329959	-0.108751	4.817734
560.864869	8000.474444	13.334963	-0.108728	4.817735
560.650780	8000.551482	13.339968	-0.108688	4.817758
561.062148	8000.464677	13.344973	-0.108764	4.817731
560.738487	8000.439876	13.349978	-0.108704	4.817725
560.933948	8000.541920	13.354983	-0.108740	4.817754
561.092675	8000.435579	13.359987	-0.108770	4.817722
560.823609	8000.561397	13.364992	-0.108720	4.817761
560.813335	8000.461014	13.369997	-0.108718	4.817731
560.683273	8000.573048	13.375002	-0.108694	4.817765
560.990435	8000.542742	13.380007	-0.108751	4.817754
560.953224	8000.533753	13.385011	-0.108744	4.817752
560.914550	8000.523687	13.390016	-0.108737	4.817749
561.027744	8000.432503	13.395021	-0.108758	4.817722
560.505845	8000.443828	13.400026	-0.108660	4.817727
560.790193	8000.479653	13.405031	-0.108713	4.817737
560.751670	8000.426333	13.410035	-0.108706	4.817721
560.907987	8000.559455	13.415040	-0.108735	4.817760
560.877384	8000.458773	13.420045	-0.108729	4.817730
560.820771	8000.484316	13.425050	-0.108719	4.817738
560.890380	8000.554971	13.430055	-0.108732	4.817758
560.809133	8000.492582	13.435059	-0.108717	4.817740
560.809137	8000.405011	13.440064	-0.108717	4.817714
560.834272	8000.562582	13.445069	-0.108721	4.817761
560.868473	8000.450191	13.450074	-0.108728	4.817728
561.067380	8000.540681	13.455079	-0.108765	4.817753
561.396624	8000.548682	13.460083	-0.108826	4.817754
561.172804	8000.516905	13.465088	-0.108784	4.817746
561.063965	8000.463606	13.470093	-0.108764	4.817731
561.178274	8000.532808	13.475098	-0.108785	4.817751
561.288057	8000.517538	13.480103	-0.108806	4.817746
560.893248	8000.461094	13.485107	-0.108732	4.817731
560.892767	8000.557095	13.490112	-0.108732	4.817759
561.000473	8000.461610	13.495117	-0.108752	4.817730
561.196965	8000.523578	13.500122	-0.108789	4.817748
560.985344	8000.539459	13.505127	-0.108749	4.817753
561.174626	8000.565449	13.510131	-0.108784	4.817760
560.778374	8000.382377	13.515136	-0.108711	4.817708
560.939692	8000.553554	13.520141	-0.108741	4.817758
560.781056	8000.565993	13.525146	-0.108711	4.817762
561.030716	8000.467317	13.530151	-0.108758	4.817732
561.135486	8000.477295	13.535155	-0.108777	4.817734
560.792689	8000.575654	13.540160	-0.108713	4.817765
561.073395	8000.439453	13.545165	-0.108765	4.817724
560.855727	8000.566026	13.550170	-0.108725	4.817762
560.977263	8000.486570	13.555175	-0.108747	4.817738
561.153681	8000.475444	13.560179	-0.108780	4.817734
561.139606	8000.548035	13.565184	-0.108778	4.817755
560.936066	8000.365683	13.570189	-0.108740	4.817702
561.034033	8000.552811	13.575194	-0.108758	4.817757
560.841438	8000.552090	13.580199	-0.108722	4.817758
560.529219	8000.312227	13.585203	-0.108664	4.817688
560.809346	8000.446110	13.590208	-0.108716	4.817727
560.682311	8000.471674	13.595213	-0.108692	4.817735
560.879226	8000.442912	13.600218	-0.108729	4.817725
560.718149	8000.448985	13.605223	-0.108699	4.817728
560.622063	8000.464453	13.610227	-0.108681	4.817733
560.886090	8000.422962	13.615232	-0.108730	4.817719
561.120925	8000.532971	13.620237	-0.108774	4.817751
561.198592	8000.532000	13.625242	-0.108788	4.817750
561.122809	8000.540380	13.630247	-0.108774	4.817753
561.110736	8000.445246	13.635251	-0.108772	4.817725
561.143996	8000.541743	13.640256	-0.108778	4.817753
561.032934	8000.330153	13.645261	-0.108757	4.817691
560.793638	8000.288656	13.650266	-0.108713	4.817680
560.583768	8000.387912	13.655271	-0.108674	4.817710
560.877126	8000.469237	13.660275	-0.108728	4.817733
560.975671	8000.446417	13.665280	-0.108747	4.817726
561.237932	8000.580041	13.670285	-0.108796	4.817764
560.811788	8000.449282	13.675290	-0.108716	4.817728
561.221591	8000.435253	13.680295	-0.108792	4.817722
561.160308	8000.567289	13.685299	-0.108781	4.817761
560.977124	8000.557211	13.690304	-0.108747	4.817759
560.866677	8000.454301	13.695309	-0.108726	4.817729
560.865170	8000.558728	13.700314	-0.108726	4.817760
560.893312	8000.515882	13.705319	-0.108731	4.817747
560.796220	8000.534501	13.710323	-0.108713	4.817753
561.194208	8000.527684	13.715328	-0.108787	4.817749
561.058100	8000.525683	13.720333	-0.108762	4.817749
560.938691	8000.438468	13.725338	-0.108740	4.817724
561.149360	8000.506974	13.730343	-0.108779	4.817743
561.157722	8000.546133	13.735347	-0.108780	4.817755
560.978786	8000.535062	13.740352	-0.108747	4.817752
561.156314	8000.566155	13.745357	-0.108780	4.817761
561.323274	8000.457824	13.750362	-0.108811	4.817728
561.067263	8000.551127	13.755367	-0.108763	4.817757
561.181149	8000.546468	13.760371	-0.108785	4.817755
560.924272	8000.513151	13.765376	-0.108737	4.817746
560.957041	8000.435557	13.770381	-0.108743	4.817723
561.084345	8000.549261	13.775386	-0.108767	4.817756
561.077140	8000.515392	13.780391	-0.108765	4.817746
561.193622	8000.562469	13.785395	-0.108787	4.817759
561.122799	8000.516059	13.790400	-0.108774	4.817746
561.186582	8000.529655	13.795405	-0.108785	4.817750
561.204367	8000.526749	13.800410	-0.108789	4.817749
561.104585	8000.490465	13.805415	-0.108770	4.817739
561.114008	8000.541245	13.810419	-0.108772	4.817753
561.138913	8000.524728	13.815424	-0.108776	4.817748
561.097569	8000.558936	13.820429	-0.108769	4.817759
561.065664	8000.456124	13.825434	-0.108763	4.817729
561.140417	8000.554286	13.830439	-0.108777	4.817757
561.464400	8000.568541	13.835443	-0.108837	4.817760
561.084213	8000.526026	13.840448	-0.108766	4.817749
561.235425	8000.500814	13.845453	-0.108794	4.817741
561.179842	8000.561189	13.850458	-0.108784	4.817759
561.075888	8000.444658	13.855463	-0.108765	4.817725
561.176483	8000.569577	13.860467	-0.108783	4.817762
561.041303	8000.557039	13.865472	-0.108758	4.817758
560.951087	8000.362636	13.870477	-0.108741	4.817701
561.048201	8000.553971	13.875482	-0.108759	4.817758
561.015458	8000.451148	13.880487	-0.108753	4.817727
561.139296	8000.462460	13.885491	-0.108776	4.817730
561.004572	8000.439379	13.890496	-0.108751	4.817724
560.932337	8000.466803	13.895501	-0.108738	4.817732
561.218627	8000.576513	13.900506	-0.108791	4.817763
560.989439	8000.446537	13.905511	-0.108748	4.817726
561.296339	8000.476364	13.910515	-0.108805	4.817734
561.028130	8000.461872	13.915520	-0.108755	4.817730
561.270656	8000.575160	13.920525	-0.108801	4.817763
561.193986	8000.567702	13.925530	-0.108786	4.817761
560.767912	8000.431669	13.930535	-0.108707	4.817723
560.944539	8000.570364	13.935539	-0.108740	4.817763
561.057338	8000.442247	13.940544	-0.108761	4.817724
560.699029	8000.466524	13.945549	-0.108694	4.817733
560.959729	8000.432369	13.950554	-0.108742	4.817722
560.542801	8000.362942	13.955559	-0.108665	4.817703
560.832198	8000.483246	13.960563	-0.108719	4.817738
560.942730	8000.538675	13.965568	-0.108739	4.817753
561.054367	8000.472790	13.970573	-0.108760	4.817734
560.964774	8000.474637	13.975578	-0.108743	4.817734
561.101642	8000.460820	13.980583	-0.108769	4.817730
560.977749	8000.456888	13.985587	-0.108746	4.817729
560.768454	8000.347253	13.990592	-0.108707	4.817698
560.447677	8000.291899	13.995597	-0.108647	4.817683
561.086161	8000.361410	14.000602	-0.108766	4.817700
560.873917	8000.435310	14.005607	-0.108726	4.817723
560.632911	8000.388512	14.010611	-0.108681	4.817710
560.219815	8000.317034	14.015616	-0.108604	4.817691
560.567035	8000.413918	14.020621	-0.108669	4.817718
560.494418	8000.341107	14.025626	-0.108655	4.817697
560.624162	8000.446405	14.030631	-0.108680	4.817728
560.972353	8000.430415	14.035635	-0.108744	4.817721
560.880602	8000.464938	14.040640	-0.108727	4.817732
560.781862	8000.445550	14.045645	-0.108709	4.817727
561.001983	8000.343276	14.050650	-0.108750	4.817695
560.797545	8000.477429	14.055655	-0.108712	4.817736
560.692609	8000.341895	14.060659	-0.108692	4.817696
560.889473	8000.432353	14.065664	-0.108729	4.817722
561.106188	8000.554757	14.070669	-0.108769	4.817758
560.897507	8000.464119	14.075674	-0.108730	4.817732
561.094777	8000.438528	14.080679	-0.108767	4.817723
561.135494	8000.575228	14.085683	-0.108775	4.817763
560.936898	8000.462583	14.090688	-0.108738	4.817731
560.883270	8000.563079	14.095693	-0.108728	4.817761
560.916890	8000.436964	14.100698	-0.108734	4.817724
560.852802	8000.442351	14.105703	-0.108722	4.817725
560.706306	8000.459189	14.110707	-0.108695	4.817731
560.786154	8000.433984	14.115712	-0.108709	4.817723
560.991260	8000.474976	14.120717	-0.108748	4.817734
560.448277	8000.252827	14.125722	-0.108646	4.817671
560.164224	8000.259207	14.130727	-0.108593	4.817674
560.353225	8000.186017	14.135731	-0.108629	4.817652
560.368113	8000.441552	14.140736	-0.108631	4.817727
559.999001	8000.169210	14.145741	-0.108563	4.817648
560.390671	8000.230873	14.150746	-0.108636	4.817665
560.845683	8000.548790	14.155751	-0.108720	4.817757
560.767317	8000.456903	14.160755	-0.108706	4.817730
560.770502	8000.463278	14.165760	-0.108706	4.817732
560.166838	8000.212810	14.170765	-0.108594	4.817660
560.322296	8000.306878	14.175770	-0.108623	4.817688
560.059991	8000.327291	14.180775	-0.108574	4.817695
560.268045	8000.259657	14.185779	-0.108613	4.817674
560.171732	8000.295167	14.190784	-0.108595	4.817685
560.085297	8000.217935	14.195789	-0.108578	4.817662
560.355315	8000.321069	14.200794	-0.108629	4.817692
560.697921	8000.433712	14.205799	-0.108693	4.817724
560.809527	8000.331955	14.210803	-0.108713	4.817693
560.932923	8000.574318	14.215808	-0.108736	4.817764
560.913040	7999.312216	14.220813	-0.108732	4.817391

560.981165	7996.213966	14.225818	-0.108743	4.816473
561.223453	7990.586957	14.230823	-0.108784	4.814807
561.020498	7984.039519	14.235827	-0.108742	4.812868
561.044178	7976.738386	14.240832	-0.108741	4.810705
560.798684	7969.126143	14.245837	-0.108691	4.808450
560.806245	7961.385271	14.250842	-0.108687	4.806154
560.853891	7953.419310	14.255847	-0.108691	4.803791
560.922815	7945.526942	14.260851	-0.108698	4.801448
560.863553	7937.506403	14.265856	-0.108682	4.799066
560.446318	7929.575573	14.270861	-0.108599	4.796711
560.715089	7921.531577	14.275866	-0.108644	4.794318
560.539584	7913.548878	14.280871	-0.108606	4.791945
560.641248	7905.493928	14.285875	-0.108620	4.789547
560.336837	7897.588993	14.290880	-0.108558	4.787195
560.168855	7889.432991	14.295885	-0.108521	4.784766
560.259504	7881.546074	14.300890	-0.108533	4.782415
560.237741	7873.485849	14.305895	-0.108524	4.780012
560.096201	7865.544459	14.310899	-0.108492	4.777643
559.776495	7857.518280	14.315904	-0.108427	4.775249
559.899175	7849.477092	14.320909	-0.108445	4.772847
559.994038	7841.538855	14.325914	-0.108457	4.770475
559.779001	7833.533376	14.330919	-0.108412	4.768082
559.935691	7825.505621	14.335923	-0.108436	4.765681
559.955402	7817.497147	14.340928	-0.108435	4.763285
559.793443	7809.506518	14.345933	-0.108399	4.760893
559.590716	7801.546666	14.350938	-0.108356	4.758509
559.910583	7793.500118	14.355943	-0.108411	4.756097
559.736585	7785.461193	14.360947	-0.108373	4.753687
559.524107	7777.503055	14.365952	-0.108328	4.751300
559.911105	7769.393261	14.370957	-0.108395	4.748865
560.012276	7761.479312	14.375962	-0.108408	4.746488
559.571312	7753.381749	14.380967	-0.108321	4.744056
559.536487	7745.490284	14.385971	-0.108309	4.741684
559.488068	7737.470877	14.390976	-0.108295	4.739273
559.502624	7729.483058	14.395981	-0.108293	4.736869
559.329679	7721.382737	14.400986	-0.108255	4.734431
559.120388	7713.471863	14.405991	-0.108211	4.732048
559.233655	7705.470134	14.410995	-0.108227	4.729637
558.680693	7697.485170	14.416000	-0.108119	4.727230
558.773021	7689.388045	14.421005	-0.108131	4.724787
558.525619	7681.527458	14.426010	-0.108079	4.722415
558.846668	7673.427739	14.431015	-0.108134	4.719968
559.145483	7665.392906	14.436019	-0.108184	4.717540
559.377938	7657.380267	14.441024	-0.108222	4.715117
559.147392	7649.389454	14.446029	-0.108174	4.712701
559.031698	7641.459218	14.451034	-0.108147	4.710301
559.049258	7633.451373	14.456039	-0.108145	4.707877
559.058060	7625.385786	14.461043	-0.108142	4.705434
558.651040	7617.470449	14.466048	-0.108061	4.703035
558.289627	7609.444273	14.471053	-0.107988	4.700602
558.762778	7601.435824	14.476058	-0.108071	4.698171
558.688850	7593.398903	14.481063	-0.108052	4.695732
558.542747	7585.443967	14.486067	-0.108020	4.693316
558.257136	7577.512093	14.491072	-0.107961	4.690906
558.472152	7569.422265	14.496077	-0.107996	4.688446
558.417460	7561.443262	14.501082	-0.107981	4.686019
558.445774	7553.356956	14.506087	-0.107981	4.683558
558.343751	7545.457900	14.511091	-0.107956	4.681153
558.277919	7537.443213	14.516096	-0.107939	4.678711
558.149310	7529.460186	14.521101	-0.107910	4.676278
558.350191	7521.411763	14.526106	-0.107942	4.673823
558.431725	7513.344655	14.531111	-0.107952	4.671362
558.042022	7505.346976	14.536115	-0.107874	4.668920
557.840538	7497.421540	14.541120	-0.107831	4.666499
557.800478	7489.379141	14.546125	-0.107819	4.664041
558.040203	7481.459988	14.551130	-0.107858	4.661620
558.252472	7473.331599	14.556135	-0.107892	4.659133
558.411891	7465.422529	14.561139	-0.107917	4.656712
558.214475	7457.382464	14.566144	-0.107875	4.654249
558.200602	7449.402998	14.571149	-0.107867	4.651804
558.261460	7441.374888	14.576154	-0.107873	4.649343
558.039292	7433.415875	14.581159	-0.107826	4.646901
557.488913	7425.366330	14.586163	-0.107719	4.644431
557.329525	7417.509525	14.591168	-0.107684	4.642018
557.550660	7409.332942	14.596173	-0.107720	4.639506
557.505713	7401.459175	14.601178	-0.107706	4.637085
557.424723	7393.359193	14.606183	-0.107686	4.634594
557.720923	7385.412601	14.611187	-0.107736	4.632149
557.393145	7377.402463	14.616192	-0.107669	4.629682
557.448225	7369.378246	14.621197	-0.107674	4.627210
557.751347	7361.310504	14.626202	-0.107726	4.624723
557.635792	7353.400245	14.631207	-0.107699	4.622284
557.599565	7345.355540	14.636211	-0.107687	4.619802
557.364178	7337.430715	14.641216	-0.107638	4.617355
557.185559	7329.349441	14.646221	-0.107599	4.614859
557.172891	7321.370275	14.651226	-0.107592	4.612393
557.434294	7313.275738	14.656231	-0.107635	4.609890
557.111868	7305.353240	14.661235	-0.107570	4.607438
556.802401	7297.395738	14.666240	-0.107507	4.604975
556.596931	7289.426232	14.671245	-0.107464	4.602506
556.776770	7281.386494	14.676250	-0.107492	4.600015
556.321866	7273.439510	14.681255	-0.107402	4.597550
556.363236	7265.350524	14.686259	-0.107404	4.595041
556.454756	7257.394486	14.691264	-0.107416	4.592571
556.545206	7249.310049	14.696269	-0.107428	4.590061
556.297052	7241.395000	14.701274	-0.107376	4.587601
556.199291	7233.311041	14.706279	-0.107353	4.585087
556.698414	7225.292295	14.711283	-0.107441	4.582593
556.494338	7217.328915	14.716288	-0.107397	4.580114
556.497874	7209.285806	14.721293	-0.107393	4.577610
556.693955	7201.276247	14.726298	-0.107424	4.575114
556.210512	7193.354426	14.731303	-0.107329	4.572644
556.129373	7185.281935	14.736307	-0.107308	4.570126
555.969254	7177.319356	14.741312	-0.107273	4.567640
556.131272	7169.266456	14.746317	-0.107298	4.565126
556.028834	7161.411241	14.751322	-0.107274	4.562671
555.902585	7153.292873	14.756327	-0.107245	4.560133
555.621638	7145.345665	14.761331	-0.107188	4.557647
555.989961	7137.287136	14.766336	-0.107251	4.555125
556.002178	7129.294047	14.771341	-0.107248	4.552622
556.264718	7121.248896	14.776346	-0.107292	4.550102
556.127629	7113.293490	14.781351	-0.107261	4.547608
555.767172	7105.263487	14.786355	-0.107189	4.545089
555.830345	7097.352366	14.791360	-0.107195	4.542606
555.911096	7089.269488	14.796365	-0.107205	4.540068
555.907776	7081.328841	14.801370	-0.107199	4.537573
556.107631	7073.229140	14.806375	-0.107231	4.535028
555.917530	7065.299789	14.811379	-0.107190	4.532533
556.035226	7057.230531	14.816384	-0.107207	4.529994
555.715302	7049.251716	14.821389	-0.107142	4.527481
555.459235	7041.262055	14.826394	-0.107089	4.524963
555.034820	7033.346750	14.831399	-0.107005	4.522467
555.298265	7025.267510	14.836403	-0.107049	4.519919
555.404356	7017.295055	14.841408	-0.107063	4.517403
555.518900	7009.228084	14.846413	-0.107080	4.514856
555.769836	7001.219642	14.851418	-0.107121	4.512327
555.530797	6993.215456	14.856423	-0.107071	4.509796
555.035122	6985.240137	14.861427	-0.106974	4.507272
554.922086	6977.238968	14.866432	-0.106947	4.504739
555.081617	6969.193201	14.871437	-0.106972	4.502192
554.805923	6961.242232	14.876442	-0.106915	4.499672
555.034481	6953.220509	14.881447	-0.106953	4.497130
554.682558	6945.222388	14.886451	-0.106882	4.494592
554.600354	6937.244612	14.891456	-0.106861	4.492059
554.852391	6929.176178	14.896461	-0.106903	4.489498
554.776546	6921.223110	14.901466	-0.106884	4.486971
554.438503	6913.181427	14.906471	-0.106816	4.484413
554.630292	6905.215668	14.911475	-0.106846	4.481880
554.750860	6897.178720	14.916480	-0.106863	4.479322
554.388456	6889.256156	14.921485	-0.106791	4.476798
554.279590	6881.186157	14.926490	-0.106765	4.474226
554.158254	6873.251206	14.931495	-0.106737	4.471695
554.748887	6865.090509	14.936499	-0.106842	4.469094
554.800043	6857.154561	14.941504	-0.106846	4.466562
554.899902	6849.091503	14.946509	-0.106859	4.463987
554.939023	6841.240944	14.951514	-0.106862	4.461478
554.663429	6833.216555	14.956519	-0.106805	4.458911
554.729715	6825.179483	14.961523	-0.106812	4.456340
554.898781	6817.178736	14.966528	-0.106838	4.453780
554.809447	6809.142364	14.971533	-0.106816	4.451206
554.457723	6801.206994	14.976538	-0.106746	4.448661
554.533529	6793.129895	14.981543	-0.106755	4.446071
554.807877	6785.139164	14.986547	-0.106800	4.443509
554.568102	6777.165530	14.991552	-0.106751	4.440948
554.245532	6769.179398	14.996557	-0.106685	4.438381
554.611181	6761.151483	15.001562	-0.106748	4.435802
554.355591	6753.160118	15.006567	-0.106695	4.433231
554.398706	6745.141620	15.011571	-0.106698	4.430651
554.444770	6737.163603	15.016576	-0.106701	4.428083
554.142816	6729.110587	15.021581	-0.106640	4.425487
554.141420	6721.189177	15.026586	-0.106635	4.422933
554.058581	6713.138229	15.031591	-0.106614	4.420336
554.181647	6705.151459	15.036595	-0.106632	4.417759
554.091226	6697.141036	15.041600	-0.106609	4.415172
553.955287	6689.126476	15.046605	-0.106579	4.412582
554.161291	6681.096265	15.051610	-0.106612	4.409987
553.840289	6673.156181	15.056615	-0.106547	4.407416
553.666656	6665.072648	15.061619	-0.106509	4.404799
553.615610	6657.174894	15.066624	-0.106495	4.402241
553.782669	6649.059178	15.071629	-0.106521	4.399611
553.742068	6641.156118	15.076634	-0.106508	4.397049
553.568188	6633.098549	15.081639	-0.106470	4.394433
553.729665	6625.095335	15.086643	-0.106495	4.391836
553.573442	6617.082633	15.091648	-0.106461	4.389232
553.330725	6609.156109	15.096653	-0.106410	4.386655
553.649026	6601.093002	15.101658	-0.106464	4.384034
553.449432	6593.196235	15.106663	-0.106422	4.381463
553.271257	6585.137941	15.111667	-0.106383	4.378838
553.417418	6577.184442	15.116672	-0.106406	4.376248
553.485102	6569.122290	15.121677	-0.106413	4.373620
553.324353	6561.145184	15.126682	-0.106378	4.371017
552.993618	6553.156303	15.131687	-0.106311	4.368407
552.770005	6545.175855	15.136691	-0.106264	4.365800
553.114181	6537.175059	15.141696	-0.106323	4.363187
552.599647	6529.198912	15.146701	-0.106222	4.360576
552.810857	6521.238093	15.151706	-0.106256	4.357973
552.758538	6513.195129	15.156711	-0.106241	4.355339
552.690689	6505.143102	15.161715	-0.106223	4.352701
552.601447	6497.200250	15.166720	-0.106201	4.350097
552.753098	6489.115098	15.171725	-0.106224	4.347447
552.548995	6481.144492	15.176730	-0.106181	4.344829
552.444650	6473.205057	15.181735	-0.106156	4.342222
552.423574	6465.187817	15.186739	-0.106147	4.339587
552.425700	6457.203412	15.191744	-0.106142	4.336962
552.255429	6449.162349	15.196749	-0.106105	4.334316
552.468119	6441.197987	15.201754	-0.106140	4.331696
552.305856	6433.129633	15.206759	-0.106104	4.329037
552.532577	6425.138580	15.211763	-0.106141	4.326405
552.422002	6417.167896	15.216768	-0.106115	4.323776
552.232168	6409.237118	15.221773	-0.106075	4.321157
552.377342	6401.251146	15.226778	-0.106097	4.318522
552.215263	6393.219856	15.231783	-0.106061	4.315867
552.341245	6385.208223	15.236787	-0.106079	4.313220
552.263019	6377.186705	15.241792	-0.106060	4.310566
551.766321	6369.234352	15.246797	-0.105962	4.307929
551.658115	6361.140668	15.251802	-0.105937	4.305248
551.841952	6353.231153	15.256807	-0.105966	4.302628
551.678176	6345.115961	15.261811	-0.105930	4.299936
551.567451	6337.203030	15.266816	-0.105904	4.297309
552.178847	6329.053491	15.271821	-0.106012	4.294609
552.100387	6321.128828	15.276826	-0.105993	4.291975
551.718228	6313.131618	15.281831	-0.105916	4.289314
551.748313	6305.137996	15.286835	-0.105917	4.286655
551.838659	6297.113026	15.291840	-0.105928	4.283985
551.424328	6289.220925	15.296845	-0.105846	4.281352
551.411565	6281.163770	15.301850	-0.105838	4.278667
551.714037	6273.162053	15.306855	-0.105889	4.276002
551.434596	6265.143780	15.311859	-0.105832	4.273324
551.525710	6257.154056	15.316864	-0.105844	4.270657
551.207257	6249.159216	15.321869	-0.105779	4.267983
551.090624	6241.122785	15.326874	-0.105752	4.265295
551.103810	6233.167113	15.331879	-0.105750	4.262634
551.110652	6225.092582	15.336883	-0.105746	4.259931
551.137765	6217.169826	15.341888	-0.105745	4.257278
550.995325	6209.126522	15.346893	-0.105714	4.254581
551.080476	6201.148785	15.351898	-0.105724	4.251906
551.644181	6193.031853	15.356903	-0.105824	4.249188
551.455677	6185.095376	15.361907	-0.105784	4.246521
551.081959	6177.141585	15.366912	-0.105709	4.243845
550.821959	6169.197937	15.371917	-0.105655	4.241171
550.901000	6161.169462	15.376922	-0.105665	4.238471
550.950135	6153.167377	15.381927	-0.105669	4.235778
550.652930	6145.134566	15.386931	-0.105608	4.233069
550.953682	6137.145225	15.391936	-0.105659	4.230379
550.633334	6129.167932	15.396941	-0.105594	4.227685
550.403736	6121.085785	15.401946	-0.105546	4.224955
550.215852	6113.211894	15.406951	-0.105506	4.222294
550.075050	6105.134705	15.411955	-0.105474	4.219562
550.326725	6097.154719	15.416960	-0.105516	4.216867
549.739650	6089.170395	15.421965	-0.105401	4.214159
550.000126	6081.131199	15.426970	-0.105445	4.211439
549.786906	6073.145479	15.431975	-0.105400	4.208731
549.674256	6065.138728	15.436979	-0.105373	4.206015
549.628048	6057.191159	15.441984	-0.105360	4.203319
549.466876	6049.140318	15.446989	-0.105324	4.200584
549.553383	6041.134417	15.451994	-0.105335	4.197865
549.556247	6033.133689	15.456999	-0.105331	4.195146
548.992351	6025.128585	15.462003	-0.105220	4.192416
549.045635	6017.078919	15.467008	-0.105225	4.189677
549.274669	6009.070733	15.472013	-0.105262	4.186952
548.915234	6001.093109	15.477018	-0.105190	4.184229
549.351324	5993.074505	15.482023	-0.105266	4.181500
549.175400	5985.031640	15.487027	-0.105228	4.178753
549.098455	5977.153416	15.492032	-0.105209	4.176062
548.972289	5969.101170	15.497037	-0.105180	4.173309
548.783990	5961.135871	15.502042	-0.105140	4.170583
549.055234	5953.104117	15.507047	-0.105185	4.167838
548.372102	5945.138533	15.512051	-0.105052	4.165103
548.711642	5937.144961	15.517056	-0.105110	4.162368
548.842215	5929.049254	15.522061	-0.105129	4.159594
548.714151	5921.150114	15.527066	-0.105100	4.156883
548.431055	5913.128128	15.532071	-0.105042	4.154125
548.541058	5905.160954	15.537075	-0.105058	4.151390
548.928955	5897.079017	15.542080	-0.105125	4.148616
548.773193	5889.069412	15.547085	-0.105090	4.145859
548.513030	5881.127078	15.552090	-0.105037	4.143122
548.546834	5873.133927	15.557095	-0.105038	4.140370
548.644480	5865.119263	15.562099	-0.105051	4.137609
548.540818	5857.134633	15.567104	-0.105026	4.134853
548.073148	5849.167245	15.572109	-0.104934	4.132098
548.587173	5841.052623	15.577114	-0.105024	4.129302
547.916440	5833.212232	15.582119	-0.104894	4.126584
548.081681	5825.091797	15.587123	-0.104920	4.123778
548.620367	5817.132058	15.592128	-0.105015	4.121030
548.435849	5809.119665	15.597133	-0.104975	4.118253
548.131414	5801.176849	15.602138	-0.104913	4.115497
548.220548	5793.153962	15.607143	-0.104925	4.112716
548.506798	5785.071196	15.612147	-0.104973	4.109915
548.224309	5777.130342	15.617152	-0.104915	4.107154
548.510046	5769.029682	15.622157	-0.104963	4.104343
548.701480	5761.120420	15.627162	-0.104993	4.101596
548.490554	5753.167854	15.632167	-0.104949	4.098826
547.984072	5745.181514	15.637171	-0.104849	4.096039
547.845279	5737.203932	15.642176	-0.104818	4.093257
547.807008	5729.129299	15.647181	-0.104806	4.090441
548.126815	5721.129771	15.652186	-0.104860	4.087655
548.159923	5713.065942	15.657191	-0.104861	4.084840
547.956813	5705.155830	15.662195	-0.104818	4.082074
547.907054	5697.144861	15.667200	-0.104804	4.079272
547.451559	5689.216905	15.672205	-0.104714	4.076492
547.635255	5681.168087	15.677210	-0.104742	4.073677
547.951068	5673.112109	15.682215	-0.104796	4.070860
547.899085	5665.093069	15.687219	-0.104781	4.068048
547.624550	5657.185082	15.692224	-0.104725	4.065269
547.391165	5649.182195	15.697229	-0.104676	4.062456
547.312505	5641.165036	15.702234	-0.104656	4.059639
547.451837	5633.171671	15.707239	-0.104677	4.056831
547.488737	5625.117223	15.712243	-0.104679	4.053998
547.581106	5617.128057	15.717248	-0.104691	4.051187
547.198606	5609.138436	15.722253	-0.104614	4.048366
547.712694	5601.065889	15.727258	-0.104704	4.045529
547.862511	5593.115603	15.732263	-0.104727	4.042726
547.104970	5585.196533	15.737267	-0.104581	4.039919
547.494455	5577.184918	15.742272	-0.104648	4.037095
546.928079	5569.169959	15.747277	-0.104538	4.034253
546.853125	5561.171636	15.752282	-0.104518	4.031422
546.859272	5553.131261	15.757287	-0.104514	4.028575
546.586275	5545.128502	15.762291	-0.104458	4.025736
546.963202	5537.111853	15.767296	-0.104523	4.022900
546.759937	5529.111178	15.772301	-0.104480	4.020058
546.941382	5521.121590	15.777306	-0.104509	4.017225
546.839845	5513.128550	15.782311	-0.104484	4.014383
546.497736	5505.170701	15.787315	-0.104416	4.011549
546.896782	5497.151992	15.792320	-0.104485	4.008702
546.774854	5489.146289	15.797325	-0.104457	4.005850
546.062341	5481.236881	15.802330	-0.104319	4.003020
546.026259	5473.225629	15.807335	-0.104307	4.000163
546.260224	5465.170723	15.812339	-0.104345	3.997293
546.406716	5457.167584	15.817344	-0.104367	3.994438
546.371714	5449.176948	15.822349	-0.104355	3.991583
546.191153	5441.171905	15.827354	-0.104317	3.988717
545.833534	5433.229108	15.832359	-0.104245	3.985869
545.399003	5425.269682	15.837363	-0.104159	3.983011
546.067167	5417.143846	15.842368	-0.104278	3.980111
546.061984	5409.166676	15.847373	-0.104272	3.977250
546.019492	5401.175321	15.852378	-0.104258	3.974382
546.053141	5393.196486	15.857383	-0.104259	3.971517
545.956466	5385.146397	15.862387	-0.104236	3.968622
545.893376	5377.216865	15.867392	-0.104219	3.965770
545.421938	5369.248137	15.872397	-0.104126	3.962893
545.817747	5361.181021	15.877402	-0.104195	3.959995
545.895581	5353.242795	15.882407	-0.104204	3.957135
545.463688	5345.188577	15.887411	-0.104118	3.954222
545.668394	5337.229699	15.892416	-0.104151	3.951353
545.586137	5329.192432	15.897421	-0.104131	3.948448
545.767956	5321.140909	15.902426	-0.104159	3.945541
546.093283	5313.181164	15.907431	-0.104215	3.942668
545.667688	5305.168666	15.912435	-0.104130	3.939759
545.067898	5297.314150	15.917440	-0.104013	3.936903
545.498728	5289.211438	15.922445	-0.104088	3.933973
545.638715	5281.180271	15.927450	-0.104109	3.931062
545.898286	5273.160010	15.932455	-0.104152	3.928154
545.750721	5265.158921	15.937459	-0.104119	3.925244
545.527474	5257.253591	15.942464	-0.104073	3.922366
545.464907	5249.204283	15.947469	-0.104056	3.919435
545.357707	5241.272200	15.952474	-0.104031	3.916545
545.200050	5233.280168	15.957479	-0.103996	3.913629
545.400799	5225.179435	15.962483	-0.104028	3.910678
545.529006	5217.205716	15.967488	-0.104047	3.907771
545.206990	5209.225908	15.972493	-0.103982	3.904850
545.401343	5201.216156	15.977498	-0.104012	3.901925
545.456913	5193.231700	15.982503	-0.104018	3.899006
545.411300	5185.233918	15.987507	-0.104004	3.896077
545.370605	5177.223170	15.992512	-0.103991	3.893141
545.315144	5169.224394	15.997517	-0.103975	3.890208
545.120514	5161.241788	16.002522	-0.103934	3.887275
545.166400	5153.254746	16.007527	-0.103937	3.884343
545.147275	5145.278974	16.012531	-0.103929	3.881412
545.055230	5137.283539	16.017536	-0.103906	3.878470
544.751439	5129.321137	16.022541	-0.103844	3.875533
544.811988	5121.216835	16.027546	-0.103850	3.872549
544.590334	5113.200445	16.032551	-0.103804	3.869590
544.454450	5105.215128	16.037555	-0.103773	3.866642
544.340709	5097.250794	16.042560	-0.103747	3.863699
544.191213	5089.307256	16.047565	-0.103714	3.860761
543.712271	5081.326737	16.052570	-0.103619	3.857801
543.861851	5073.309514	16.057575	-0.103642	3.854837
543.565494	5065.289085	16.062579	-0.103582	3.851861
543.588417	5057.261067	16.067584	-0.103581	3.848886
543.276735	5049.277676	16.072589	-0.103517	3.845919
543.725675	5041.255408	16.077594	-0.103596	3.842951
543.754056	5033.314533	16.082599	-0.103596	3.840002
543.725751	5025.311657	16.087603	-0.103585	3.837026
543.753330	5017.285775	16.092608	-0.103585	3.834041
543.990913	5009.305098	16.097613	-0.103624	3.831075
544.038838	5001.244378	16.102618	-0.103628	3.828072
543.965004	4993.255656	16.107623	-0.103609	3.825092
543.883706	4985.273636	16.112627	-0.103589	3.822111
544.343056	4977.226020	16.117632	-0.103669	3.819116
544.210520	4969.332122	16.122637	-0.103639	3.816162
543.774617	4961.360551	16.127642	-0.103553	3.813171
544.036536	4953.298186	16.132647	-0.103596	3.810158
543.746520	4945.307421	16.137651	-0.103537	3.807158
543.428080	4937.353917	16.142656	-0.103472	3.804169
543.399600	4929.386114	16.147661	-0.103462	3.801178
543.548862	4921.310045	16.152666	-0.103484	3.798149
543.275233	4913.382933	16.157671	-0.103428	3.795163
543.154265	4905.342605	16.162675	-0.103400	3.792136
543.505120	4897.319920	16.167680	-0.103461	3.789124
543.466405	4889.312270	16.172685	-0.103448	3.786106
543.128410	4881.361584	16.177690	-0.103380	3.783101
543.165462	4873.383644	16.182695	-0.103382	3.780091
543.086433	4865.367121	16.187699	-0.103362	3.777062
543.074626	4857.366137	16.192704	-0.103354	3.774037
543.081873	4849.340698	16.197709	-0.103350	3.771002
543.104239	4841.352113	16.202714	-0.103349	3.767978
542.985284	4833.380379	16.207719	-0.103322	3.764955
542.657189	4825.430630	16.212723	-0.103256	3.761933
542.845890	4817.404072	16.217728	-0.103285	3.758892
542.355004	4809.467704	16.222733	-0.103189	3.755866
542.624578	4801.403833	16.227738	-0.103234	3.752807
542.834011	4793.382218	16.232743	-0.103268	3.749761
542.043858	4785.499259	16.237747	-0.103115	3.746740
542.134191	4777.448262	16.242752	-0.103127	3.743675
541.976067	4769.469592	16.247757	-0.103092	3.740628
542.263428	4761.428931	16.252762	-0.103140	3.737567
542.235537	4753.412517	16.257767	-0.103130	3.734504
542.148137	4745.407345	16.262771	-0.103108	3.731442
542.166682	4737.417447	16.267776	-0.103107	3.728385
542.000531	4729.441984	16.272781	-0.103070	3.725327
541.865530	4721.458912	16.277786	-0.103040	3.722265
541.860776	4713.478872	16.282791	-0.103034	3.719204
542.042295	4705.498119	16.287795	-0.103063	3.716145
541.985669	4697.428181	16.292800	-0.103047	3.713043
541.534899	4689.452607	16.297805	-0.102958	3.709965
541.402615	4681.441778	16.302810	-0.102928	3.706879
541.497832	4673.432368	16.307815	-0.102940	3.703797
541.241853	4665.462592	16.312819	-0.102887	3.700718
541.494017	4657.447979	16.317824	-0.102929	3.697633
541.307591	4649.441721	16.322829	-0.102889	3.694536
541.656591	4641.425023	16.327834	-0.102949	3.691448
541.628044	4633.431338	16.332839	-0.102938	3.688355
541.251688	4625.467776	16.337843	-0.102863	3.685263
541.409473	4617.501614	16.342848	-0.102887	3.682181
541.592577	4609.442153	16.347853	-0.102916	3.679061
541.325590	4601.503629	16.352858	-0.102861	3.675973
541.762341	4593.475800	16.357863	-0.102937	3.672867
541.426157	4585.472000	16.362867	-0.102869	3.669747
540.853499	4577.590009	16.367872	-0.102758	3.666665
540.767014	4569.562923	16.372877	-0.102736	3.663537
541.200011	4561.454933	16.377882	-0.102812	3.660389
540.865884	4553.581895	16.382887	-0.102744	3.657309
540.169428	4545.636003	16.387891	-0.102609	3.654188
540.792731	4537.542512	16.392896	-0.102720	3.651043
540.690034	4529.521418	16.397901	-0.102696	3.647903
541.166541	4521.452502	16.402906	-0.102779	3.644758
541.039971	4513.605426	16.407911	-0.102750	3.641681
539.866918	4505.718302	16.412915	-0.102527	3.638556
540.417923	4497.577177	16.417920	-0.102624	3.635377
540.527640	4489.586906	16.422925	-0.102639	3.632242
540.698047	4481.517424	16.427930	-0.102666	3.629074
540.671408	4473.577568	16.432935	-0.102656	3.625950
540.796178	4465.568020	16.437939	-0.102674	3.622799
540.757970	4457.595230	16.442944	-0.102661	3.619656
540.547405	4449.644093	16.447949	-0.102617	3.616514
540.231874	4441.622921	16.452954	-0.102553	3.613338
540.187736	4433.652605	16.457959	-0.102539	3.610187
539.931825	4425.678509	16.462963	-0.102487	3.607026
540.088967	4417.596510	16.467968	-0.102510	3.603832
540.096173	4409.642756	16.472973	-0.102507	3.600681
539.974566	4401.665199	16.477978	-0.102479	3.597514
540.324240	4393.605330	16.482983	-0.102539	3.594325
539.993587	4385.683105	16.487987	-0.102472	3.591168
540.090623	4377.633051	16.492992	-0.102485	3.587970
539.804820	4369.666104	16.497997	-0.102426	3.584792
539.628406	4361.703783	16.503002	-0.102388	3.581615
539.676767	4353.728093	16.508007	-0.102392	3.578437
538.877099	4345.794129	16.513011	-0.102238	3.575247
538.910190	4337.750295	16.518016	-0.102239	3.572036
539.793205	4329.587170	16.523021	-0.102398	3.568799
539.779233	4321.621247	16.528026	-0.102390	3.565611
539.599813	4313.709130	16.533031	-0.102351	3.562437
539.322977	4305.725041	16.538035	-0.102295	3.559229
538.953234	4297.818278	16.543040	-0.102221	3.556046
539.521839	4289.663808	16.548045	-0.102321	3.552788
539.230920	4281.661532	16.553050	-0.102262	3.549563
539.741649	4273.635368	16.558055	-0.102352	3.546350
539.538468	4265.655789	16.563059	-0.102309	3.543131
539.059839	4257.780433	16.568064	-0.102214	3.539943
539.361288	4249.726701	16.573069	-0.102265	3.536703
539.189146	4241.741221	16.578074	-0.102228	3.533474
539.465408	4233.742595	16.583079	-0.102274	3.530250
539.272665	4225.789571	16.588083	-0.102233	3.527027
539.141615	4217.770549	16.593088	-0.102203	3.523777
538.665650	4209.882706	16.598093	-0.102110	3.520565
539.292689	4201.739782	16.603098	-0.102221	3.517282
539.120341	4193.783166	16.608103	-0.102184	3.514047
539.087550	4185.804654	16.613107	-0.102172	3.510803
539.101986	4177.776138	16.618112	-0.102170	3.507538
539.091228	4169.760137	16.623117	-0.102163	3.504275
538.956698	4161.837147	16.628122	-0.102132	3.501042
538.966235	4153.845933	16.633127	-0.102129	3.497783
538.967232	4145.824624	16.638131	-0.102124	3.494508
538.913172	4137.844976	16.643136	-0.102108	3.491246
538.655306	4129.875247	16.648141	-0.102055	3.487978
538.931377	4121.796730	16.653146	-0.102101	3.484679
538.805344	4113.916176	16.658151	-0.102073	3.481446
539.201071	4105.857536	16.663155	-0.102141	3.478153
538.813497	4097.925319	16.668160	-0.102064	3.474884
538.946444	4089.899739	16.673165	-0.102083	3.471590
538.156824	4081.999194	16.678170	-0.101931	3.468314
538.226801	4073.925741	16.683175	-0.101939	3.464992
538.571852	4065.869561	16.688179	-0.101998	3.461684
538.469391	4057.901073	16.693184	-0.101974	3.458393
538.200559	4049.950715	16.698189	-0.101918	3.455101
538.324330	4041.911916	16.703194	-0.101936	3.451783
538.156799	4033.941534	16.708199	-0.101900	3.448480
537.721393	4025.977430	16.713203	-0.101813	3.445167
538.001881	4017.954196	16.718208	-0.101860	3.441851
537.928542	4009.973675	16.723213	-0.101841	3.438537
538.267628	4001.930083	16.728218	-0.101899	3.435208
537.781200	3994.082424	16.733223	-0.101804	3.431929
537.657701	3986.031719	16.738227	-0.101775	3.428575
537.700983	3978.010326	16.743232	-0.101778	3.425235
537.451260	3970.079491	16.748237	-0.101726	3.421920
537.354104	3962.047289	16.753242	-0.101703	3.418565
537.540663	3954.048614	16.758247	-0.101733	3.415230
537.594263	3946.043433	16.763251	-0.101737	3.411884
537.282900	3938.058834	16.768256	-0.101674	3.408531
537.446263	3930.040804	16.773261	-0.101699	3.405177
537.097680	3922.121400	16.778266	-0.101629	3.401844
536.690940	3914.185854	16.783271	-0.101548	3.398498
536.472365	3906.173318	16.788275	-0.101502	3.395123
536.667798	3898.079542	16.793280	-0.101533	3.391725
537.149167	3889.983529	16.798285	-0.101618	3.388334
537.191488	3881.997268	16.803290	-0.101620	3.384969
537.135292	3874.088743	16.808295	-0.101605	3.381630
537.142853	3866.078414	16.813299	-0.101601	3.378248
537.303779	3858.068103	16.818304	-0.101626	3.374867
537.322481	3850.108223	16.823309	-0.101624	3.371499
537.267068	3842.080919	16.828314	-0.101608	3.368097
537.315647	3834.102805	16.833319	-0.101612	3.364716
537.053421	3826.211092	16.838323	-0.101558	3.361357
536.770959	3818.232943	16.843328	-0.101500	3.357956
537.132359	3810.161473	16.848333	-0.101562	3.354537
536.577867	3802.254204	16.853338	-0.101454	3.351150
536.569228	3794.261336	16.858343	-0.101447	3.347743
536.220394	3786.264006	16.863347	-0.101377	3.344318
536.258413	3778.279054	16.868352	-0.101379	3.340910
536.217753	3770.303324	16.873357	-0.101366	3.337499
536.436962	3762.212947	16.878362	-0.101402	3.334045
536.105225	3754.285917	16.883367	-0.101335	3.330636
535.789935	3746.315497	16.888371	-0.101271	3.327207
536.220635	3738.234864	16.893376	-0.101346	3.323754
536.204521	3730.311842	16.898381	-0.101337	3.320349
535.764295	3722.362970	16.903386	-0.101250	3.316913
536.039647	3714.310034	16.908391	-0.101296	3.313456
536.108970	3706.303377	16.913395	-0.101304	3.310007
535.887696	3698.343416	16.918400	-0.101258	3.306564
536.162962	3690.285058	16.923405	-0.101303	3.303094
535.978323	3682.337124	16.928410	-0.101264	3.299650
535.954407	3674.367919	16.933415	-0.101254	3.296200
535.466155	3666.427516	16.938419	-0.101158	3.292740
535.654502	3658.367401	16.943424	-0.101188	3.289251
535.737284	3650.392898	16.948429	-0.101198	3.285792
535.808746	3642.373952	16.953434	-0.101206	3.282309
535.742508	3634.430559	16.958439	-0.101189	3.278850
536.058590	3626.372489	16.963443	-0.101242	3.275352
536.120948	3618.394804	16.968448	-0.101249	3.271876
535.634847	3610.498850	16.973453	-0.101153	3.268409
535.592221	3602.455711	16.978458	-0.101140	3.264893
535.591162	3594.498023	16.983463	-0.101134	3.261411
535.429223	3586.486767	16.988467	-0.101099	3.257896
535.515562	3578.484003	16.993472	-0.101110	3.254391
535.790266	3570.496502	16.998477	-0.101156	3.250897
535.496378	3562.534157	17.003482	-0.101096	3.247386
535.382810	3554.550272	17.008487	-0.101069	3.243870
535.425143	3546.575416	17.013491	-0.101072	3.240360
535.272638	3538.623182	17.018496	-0.101038	3.236849
535.295655	3530.598131	17.023501	-0.101038	3.233308
534.922584	3522.624053	17.028506	-0.100963	3.229770
535.131034	3514.583641	17.033511	-0.100996	3.226223
534.832809	3506.618141	17.038515	-0.100936	3.222684
534.539328	3498.644197	17.043520	-0.100876	3.219137
534.885049	3490.636163	17.048525	-0.100935	3.215598
534.656112	3482.649930	17.053530	-0.100887	3.212041
534.962409	3474.588027	17.058535	-0.100939	3.208469
534.614046	3466.650673	17.063539	-0.100869	3.204921
534.505487	3458.717563	17.068544	-0.100843	3.201380
534.654287	3450.698704	17.073549	-0.100866	3.197809
534.577023	3442.672012	17.078554	-0.100846	3.194220
534.606010	3434.707658	17.083559	-0.100846	3.190660
534.587991	3426.700258	17.088563	-0.100838	3.187074
534.125777	3418.760784	17.093568	-0.100746	3.183496
533.884876	3410.854257	17.098573	-0.100696	3.179937
534.219563	3402.750173	17.103578	-0.100753	3.176311
534.267956	3394.765552	17.108583	-0.100757	3.172723
534.435697	3386.694472	17.113587	-0.100783	3.169096
533.977957	3378.838920	17.118592	-0.100693	3.165535
533.710084	3370.883995	17.123597	-0.100638	3.161934
533.706268	3362.860616	17.128602	-0.100632	3.158309
533.765112	3354.854103	17.133607	-0.100638	3.154690
534.165324	3346.786673	17.138611	-0.100707	3.151055
533.832601	3338.856985	17.143616	-0.100640	3.147445
533.785638	3330.870549	17.148621	-0.100626	3.143818
533.732126	3322.898811	17.153626	-0.100610	3.140194
533.603467	3314.930034	17.158631	-0.100581	3.136563
533.524783	3306.919689	17.163635	-0.100561	3.132911
533.757904	3298.881555	17.168640	-0.100600	3.129256
533.780162	3290.923605	17.173645	-0.100598	3.125624
533.808666	3282.932628	17.178650	-0.100599	3.121974
533.704625	3274.996297	17.183655	-0.100574	3.118337
533.243596	3267.047849	17.188659	-0.100483	3.114675
533.257895	3259.058526	17.193664	-0.100480	3.111011
533.379178	3251.027075	17.198669	-0.100498	3.107329
533.165402	3243.020542	17.203674	-0.100453	3.103638
533.063786	3235.095015	17.208679	-0.100429	3.099985
532.884146	3227.125844	17.213683	-0.100390	3.096305
532.944108	3219.099342	17.218688	-0.100396	3.092604
532.817256	3211.093293	17.223693	-0.100367	3.088900
532.392703	3203.157577	17.228698	-0.100283	3.085210
532.773004	3195.164990	17.233703	-0.100348	3.081527
532.630032	3187.168605	17.238707	-0.100316	3.077813
532.525361	3179.157861	17.243712	-0.100292	3.074089
532.948914	3171.083230	17.248717	-0.100365	3.070357
533.140863	3163.056755	17.253722	-0.100396	3.066631
533.215620	3155.129695	17.258727	-0.100404	3.062942
533.105414	3147.158311	17.263731	-0.100379	3.059219
532.957624	3139.221287	17.268736	-0.100346	3.055505
532.673346	3131.282762	17.273741	-0.100288	3.051780
532.199608	3123.312413	17.278746	-0.100194	3.048026
532.444401	3115.262817	17.283751	-0.100235	3.044264
532.102926	3107.348573	17.288755	-0.100166	3.040534
531.916239	3099.386904	17.293760	-0.100126	3.036784
531.863666	3091.386668	17.298765	-0.100111	3.033017
531.858144	3083.371601	17.303770	-0.100105	3.029241
532.079516	3075.351995	17.308775	-0.100141	3.025470
531.571386	3067.432148	17.313779	-0.100041	3.021705
532.165938	3059.349601	17.318784	-0.100146	3.017913
531.952216	3051.402356	17.323789	-0.100101	3.014140
531.581340	3043.444919	17.328794	-0.100027	3.010350
531.577824	3035.470644	17.333799	-0.100021	3.006565
531.570862	3027.477890	17.338803	-0.100015	3.002766
531.702763	3019.466732	17.343808	-0.100034	2.998961
532.133211	3011.458129	17.348813	-0.100109	2.995168
531.673115	3003.512548	17.353818	-0.100018	2.991354
531.515346	2995.537206	17.358823	-0.099983	2.987537
531.895639	2987.472154	17.363827	-0.100049	2.983699
531.791699	2979.536957	17.368832	-0.100024	2.979894
531.799208	2971.586316	17.373837	-0.100021	2.976082
531.577320	2963.591904	17.378842	-0.099974	2.972233
531.678001	2955.593317	17.383847	-0.099988	2.968393
531.567032	2947.630475	17.388851	-0.099962	2.964555
531.573291	2939.662736	17.393856	-0.099958	2.960715
531.421658	2931.730846	17.398861	-0.099924	2.956879
531.114289	2923.742945	17.403866	-0.099862	2.953003
531.005537	2915.745384	17.408871	-0.099836	2.949128
531.181928	2907.732478	17.413875	-0.099864	2.945255
531.543611	2899.700148	17.418880	-0.099926	2.941378
531.511827	2891.762990	17.423885	-0.099915	2.937520
530.972196	2883.831605	17.428890	-0.099809	2.933634
531.086051	2875.796395	17.433895	-0.099825	2.929726
530.950451	2867.849804	17.438899	-0.099795	2.925843
530.730623	2859.895637	17.443904	-0.099749	2.921947
530.537399	2851.945436	17.448909	-0.099707	2.918049
530.675512	2843.896076	17.453914	-0.099728	2.914115
530.618462	2835.887388	17.458919	-0.099712	2.910185
530.534061	2827.878602	17.463923	-0.099691	2.906248
530.399077	2819.920600	17.468928	-0.099661	2.902328
530.097762	2812.029320	17.473933	-0.099599	2.898427
529.593090	2804.049990	17.478938	-0.099500	2.894465
530.213797	2795.979573	17.483943	-0.099611	2.890515
530.405070	2787.951480	17.488947	-0.099641	2.886557
530.263924	2780.002426	17.493952	-0.099609	2.882614
530.518652	2772.018631	17.498957	-0.099652	2.878671
530.248600	2764.072589	17.503962	-0.099596	2.874712
530.513450	2756.071117	17.508967	-0.099640	2.870749
530.058906	2748.141030	17.513971	-0.099550	2.866776
530.143221	2740.117468	17.518976	-0.099561	2.862782
530.293358	2732.150736	17.523981	-0.099584	2.858814
529.933035	2724.217294	17.528986	-0.099511	2.854828
530.013604	2716.216372	17.533991	-0.099521	2.850828
530.251078	2708.177038	17.538995	-0.099560	2.846812
530.140225	2700.225915	17.544000	-0.099534	2.842814
530.177602	2692.274697	17.549005	-0.099536	2.838820
529.871564	2684.340458	17.554010	-0.099474	2.834808
529.487148	2676.419170	17.559015	-0.099397	2.830793
529.289996	2668.408736	17.564019	-0.099355	2.826738
529.607777	2660.359351	17.569024	-0.099409	2.822687
529.922823	2652.327823	17.574029	-0.099462	2.818639
529.699232	2644.371014	17.579034	-0.099415	2.814592
529.569281	2636.427243	17.584039	-0.099386	2.810551
529.492810	2628.458099	17.589043	-0.099367	2.806495
529.403373	2620.481190	17.594048	-0.099345	2.802428
529.276860	2612.542851	17.599053	-0.099316	2.798372
529.409028	2604.530410	17.604058	-0.099335	2.794289
529.358403	2596.572253	17.609063	-0.099321	2.790216
529.343171	2588.561921	17.614067	-0.099313	2.786112
528.971663	2580.635452	17.619072	-0.099238	2.782024
529.000169	2572.674006	17.624077	-0.099238	2.777936
528.603906	2564.709190	17.629082	-0.099159	2.773815
528.779403	2556.667470	17.634087	-0.099187	2.769682
528.975431	2548.673328	17.639091	-0.099218	2.765569
528.432444	2540.802211	17.644096	-0.099112	2.761469
528.694976	2532.774455	17.649101	-0.099155	2.757330
528.988943	2524.702520	17.654106	-0.099205	2.753165
528.658329	2516.783917	17.659111	-0.099138	2.749034
528.367450	2508.815080	17.664115	-0.099079	2.744873
528.751582	2500.775884	17.669120	-0.099145	2.740711
528.775274	2492.842431	17.674125	-0.099144	2.736576
528.551434	2484.881767	17.679130	-0.099097	2.732404
528.196470	2476.944270	17.684135	-0.099026	2.728231
527.965987	2468.995299	17.689139	-0.098978	2.724052
528.207485	2460.974170	17.694144	-0.099018	2.719859
527.957739	2453.049739	17.699149	-0.098966	2.715679
528.030539	2445.037831	17.704154	-0.098974	2.711467
528.451480	2436.976300	17.709159	-0.099047	2.707245
528.142343	2429.074215	17.714163	-0.098985	2.703054
527.839123	2421.128386	17.719168	-0.098923	2.698833
527.931245	2413.165014	17.724173	-0.098935	2.694622
528.111017	2405.129311	17.729178	-0.098963	2.690371
527.744984	2397.210596	17.734183	-0.098890	2.686141
527.844564	2389.242116	17.739187	-0.098903	2.681907
527.705376	2381.272489	17.744192	-0.098872	2.677651
528.133947	2373.246393	17.749197	-0.098947	2.673395
527.808464	2365.284059	17.754202	-0.098881	2.669117
527.907471	2357.299655	17.759207	-0.098894	2.664848
527.590505	2349.388827	17.764211	-0.098830	2.660584
527.347286	2341.426068	17.769216	-0.098779	2.656290
527.646541	2333.415460	17.774221	-0.098830	2.652000
527.578050	2325.411963	17.779226	-0.098812	2.647682
527.389077	2317.489574	17.784231	-0.098771	2.643392
527.511424	2309.498446	17.789235	-0.098789	2.639080
527.174128	2301.587798	17.794240	-0.098721	2.634773
526.774992	2293.665737	17.799245	-0.098641	2.630448
527.038097	2285.578920	17.804250	-0.098685	2.626072
527.055248	2277.613064	17.809255	-0.098683	2.621737
527.626240	2269.569998	17.814259	-0.098784	2.617391
527.172192	2261.677688	17.819264	-0.098695	2.613050
527.161734	2253.710600	17.824269	-0.098687	2.608691
527.078925	2245.726024	17.829274	-0.098667	2.604311
526.910450	2237.830728	17.834279	-0.098630	2.599966
526.886623	2229.865905	17.839283	-0.098621	2.595585
526.430964	2221.850105	17.844288	-0.098530	2.591139
526.616027	2213.799971	17.849293	-0.098560	2.586711
526.501479	2205.841610	17.854298	-0.098533	2.582305
526.545961	2197.881338	17.859303	-0.098536	2.577902
526.568530	2189.909558	17.864307	-0.098535	2.573483
526.414672	2181.954685	17.869312	-0.098501	2.569054
526.377139	2174.013451	17.874317	-0.098489	2.564633
526.492615	2166.039363	17.879322	-0.098505	2.560197
525.749319	2158.197419	17.884327	-0.098362	2.555765
526.223830	2150.114912	17.889331	-0.098445	2.551278
526.460774	2142.077179	17.894336	-0.098484	2.546792
526.224652	2134.197516	17.899341	-0.098435	2.542352
526.178852	2126.223087	17.904346	-0.098421	2.537865
526.301960	2118.239209	17.909351	-0.098439	2.533377
526.465948	2110.252269	17.914355	-0.098464	2.528882
526.351061	2102.286008	17.919360	-0.098437	2.524370
526.636237	2094.330495	17.924365	-0.098485	2.519886
526.239032	2086.440336	17.929370	-0.098406	2.515381
525.657478	2078.525227	17.934375	-0.098293	2.510840
526.201392	2070.434118	17.939379	-0.098389	2.506273
526.104594	2062.479179	17.944384	-0.098365	2.501729
525.915805	2054.579332	17.949389	-0.098325	2.497201
525.792324	2046.598267	17.954394	-0.098297	2.492623
525.478950	2038.679196	17.959399	-0.098233	2.488057
525.344352	2030.715740	17.964403	-0.098203	2.483472
525.223223	2022.751226	17.969408	-0.098175	2.478878
525.227499	2014.811126	17.974413	-0.098171	2.474299
524.883431	2006.874326	17.979418	-0.098102	2.469687
525.184356	1998.805297	17.984423	-0.098152	2.465039
524.879032	1990.906922	17.989427	-0.098090	2.460435
525.033561	1982.897879	17.994432	-0.098114	2.455793
525.301814	1974.896946	17.999437	-0.098159	2.451156
524.791526	1966.995116	18.004442	-0.098058	2.446508
524.954338	1959.014724	18.009447	-0.098083	2.441857
524.669716	1951.129598	18.014451	-0.098025	2.437218
524.338838	1943.166617	18.019456	-0.097958	2.432521
524.122632	1935.195797	18.024461	-0.097913	2.427819
524.271672	1927.153139	18.029466	-0.097936	2.423095
524.742400	1919.118452	18.034471	-0.098018	2.418391
524.848516	1911.168727	18.039475	-0.098032	2.413699
524.425250	1903.269413	18.044480	-0.097948	2.408987
524.787013	1895.258942	18.049485	-0.098011	2.404261
524.544521	1887.357878	18.054490	-0.097960	2.399543
524.505406	1879.404703	18.059495	-0.097948	2.394801
524.447726	1871.486243	18.064499	-0.097932	2.390069
524.348930	1863.503510	18.069504	-0.097908	2.385286
524.203000	1855.588971	18.074509	-0.097876	2.380530
524.484722	1847.557450	18.079514	-0.097923	2.375729
524.251414	1839.637077	18.084519	-0.097874	2.370943
524.150066	1831.679851	18.089523	-0.097850	2.366136
523.953263	1823.764147	18.094528	-0.097809	2.361337
523.857535	1815.832940	18.099533	-0.097786	2.356526
523.793340	1807.859734	18.104538	-0.097768	2.351683
523.920240	1799.855230	18.109543	-0.097787	2.346827
524.001368	1791.889293	18.114547	-0.097797	2.341980
523.761259	1783.966168	18.119552	-0.097747	2.337123
524.134679	1775.963235	18.124557	-0.097811	2.332257
523.648637	1768.080146	18.129562	-0.097715	2.327384
523.763178	1760.103816	18.134567	-0.097732	2.322493
523.789624	1752.146895	18.139571	-0.097731	2.317596
523.556350	1744.232024	18.144576	-0.097683	2.312693
523.734943	1736.249011	18.149581	-0.097711	2.307772
523.536213	1728.285217	18.154586	-0.097668	2.302821
523.323400	1720.377780	18.159591	-0.097624	2.297892
523.689411	1712.366000	18.164595	-0.097687	2.292938
523.460173	1704.420743	18.169600	-0.097639	2.287963
523.107785	1696.555601	18.174605	-0.097568	2.283017
522.874545	1688.630984	18.179610	-0.097519	2.278033
523.100512	1680.615697	18.184615	-0.097556	2.273021
522.909274	1672.652077	18.189619	-0.097515	2.267994
522.942926	1664.672230	18.194624	-0.097516	2.262966
522.615609	1656.784790	18.199629	-0.097450	2.257952
521.834515	1648.948587	18.204634	-0.097300	2.252920
522.302789	1640.851516	18.209639	-0.097382	2.247822
522.057830	1632.951638	18.214643	-0.097331	2.242774
521.860969	1625.022619	18.219648	-0.097289	2.237701
521.838553	1617.073820	18.224653	-0.097280	2.232618
521.659464	1609.112063	18.229658	-0.097241	2.227502
522.356142	1601.028053	18.234663	-0.097365	2.222375
521.757700	1593.222364	18.239667	-0.097249	2.217298
521.637072	1585.264598	18.244672	-0.097221	2.212154
521.781278	1577.285600	18.249677	-0.097243	2.207008
521.802089	1569.322087	18.254682	-0.097241	2.201850
521.492365	1561.438175	18.259687	-0.097179	2.196700
521.539322	1553.489330	18.264691	-0.097182	2.191529
521.147647	1545.576085	18.269696	-0.097104	2.186329
521.480863	1537.563136	18.274701	-0.097161	2.181118
521.180665	1529.666870	18.279706	-0.097100	2.175912
520.976918	1521.759110	18.284711	-0.097057	2.170695
521.400162	1513.713070	18.289715	-0.097130	2.165433
520.879394	1505.856144	18.294720	-0.097028	2.160194
521.189125	1497.876211	18.299725	-0.097081	2.154940
521.180501	1489.924013	18.304730	-0.097074	2.149661
520.855307	1482.028808	18.309735	-0.097008	2.144377
520.801903	1474.116093	18.314739	-0.096993	2.139094
520.475703	1466.209046	18.319744	-0.096927	2.133775
520.450709	1458.263181	18.324749	-0.096917	2.128446
520.603558	1450.270025	18.329754	-0.096940	2.123089
520.329993	1442.399480	18.334759	-0.096884	2.117760
520.209430	1434.453164	18.339763	-0.096857	2.112381
520.338396	1426.412270	18.344768	-0.096875	2.106948
519.928089	1418.567821	18.349773	-0.096794	2.101582
520.310094	1410.552559	18.354778	-0.096860	2.096164
519.918705	1402.677285	18.359783	-0.096782	2.090751
519.561911	1394.783467	18.364787	-0.096710	2.085315
520.267562	1386.710537	18.369792	-0.096836	2.079847
519.943352	1378.878478	18.374797	-0.096771	2.074428
520.435644	1370.850509	18.379802	-0.096857	2.068942
519.884300	1363.016755	18.384807	-0.096749	2.063469
520.317400	1355.013983	18.389811	-0.096825	2.057965
519.801031	1347.157741	18.394816	-0.096724	2.052451
519.540797	1339.280864	18.399821	-0.096670	2.046935
519.495552	1331.342680	18.404826	-0.096656	2.041382
519.124667	1323.462753	18.409831	-0.096582	2.035821
519.459455	1315.449463	18.414835	-0.096639	2.030225
519.392320	1307.507636	18.419840	-0.096621	2.024621
519.327431	1299.627860	18.424845	-0.096604	2.019047
518.605643	1291.793713	18.429850	-0.096465	2.013420
518.859582	1283.780679	18.434855	-0.096507	2.007752
519.462935	1275.743388	18.439859	-0.096614	2.002089
519.161440	1267.888423	18.444864	-0.096553	1.996444
519.415344	1259.930548	18.449869	-0.096595	1.990768
519.972009	1251.894034	18.454874	-0.096693	1.985052
519.781608	1244.065254	18.459879	-0.096652	1.979389
519.292712	1236.264163	18.464883	-0.096556	1.973697
519.440289	1228.280153	18.469888	-0.096579	1.967926
519.685513	1220.332008	18.474893	-0.096619	1.962174
519.487403	1212.460427	18.479898	-0.096577	1.956412
519.578098	1204.530409	18.484903	-0.096589	1.950622
519.383924	1196.627163	18.489907	-0.096547	1.944804
519.302156	1188.719538	18.494912	-0.096527	1.938977
519.400101	1180.798898	18.499917	-0.096540	1.933143
519.047221	1172.924444	18.504922	-0.096469	1.927275
518.900139	1165.024854	18.509927	-0.096437	1.921393
518.859155	1157.111713	18.514931	-0.096424	1.915496
519.071514	1149.137178	18.519936	-0.096458	1.909562
519.001800	1141.243546	18.524941	-0.096440	1.903639
518.705091	1133.383503	18.529946	-0.096380	1.897697
518.830693	1125.435463	18.534951	-0.096398	1.891718
518.907007	1117.512499	18.539955	-0.096407	1.885734
518.662835	1109.642529	18.544960	-0.096356	1.879733
518.538825	1101.767635	18.549965	-0.096328	1.873724
518.581711	1093.829497	18.554970	-0.096331	1.867666
518.420140	1085.937364	18.559975	-0.096295	1.861600
518.096472	1078.085168	18.564979	-0.096230	1.855525
518.019191	1070.168169	18.569984	-0.096210	1.849410
518.407383	1062.196373	18.574989	-0.096278	1.843287
518.265874	1054.336212	18.579994	-0.096246	1.837167
518.278560	1046.418352	18.584999	-0.096243	1.831001
518.478643	1038.478264	18.590003	-0.096275	1.824819
517.807243	1030.708818	18.595008	-0.096145	1.818644
517.601177	1022.834753	18.600013	-0.096102	1.812422
518.054091	1014.829782	18.605018	-0.096181	1.806156
517.679551	1007.005988	18.610023	-0.096106	1.799910
517.051134	999.246514	18.615027	-0.095984	1.793662
517.398288	991.188213	18.620032	-0.096043	1.787274
517.797662	983.225323	18.625037	-0.096112	1.780947
517.305340	975.430024	18.630042	-0.096016	1.774620
517.223285	967.529388	18.635047	-0.095995	1.768237
517.431522	959.609849	18.640051	-0.096029	1.761853
517.590585	951.697693	18.645056	-0.096053	1.755445
517.312570	943.871006	18.650061	-0.095996	1.749027
516.822793	936.066859	18.655066	-0.095900	1.742577
516.874673	928.148781	18.660071	-0.095904	1.736079
517.131995	920.217377	18.665075	-0.095947	1.729572
516.626347	912.411845	18.670080	-0.095848	1.723046
516.929487	904.488475	18.675085	-0.095899	1.716502
517.094566	896.564062	18.680090	-0.095925	1.709915
517.028348	888.704816	18.685095	-0.095907	1.703326
516.897966	880.868894	18.690099	-0.095878	1.696723
516.737483	872.995751	18.695104	-0.095843	1.690058
516.631944	865.157932	18.700109	-0.095818	1.683404
516.887707	857.237766	18.705114	-0.095860	1.676703
516.583745	849.414147	18.710119	-0.095799	1.669981
516.467499	841.581517	18.715123	-0.095772	1.663250
516.669640	833.666972	18.720128	-0.095804	1.656464
516.763253	825.801527	18.725133	-0.095817	1.649678
516.321184	818.019872	18.730138	-0.095729	1.642863
516.279796	810.162184	18.735143	-0.095716	1.636009
515.799015	802.362859	18.740147	-0.095622	1.629115
515.994740	794.410104	18.745152	-0.095653	1.622152
515.912570	786.572488	18.750157	-0.095633	1.615222
516.188756	778.655462	18.755162	-0.095679	1.608242
516.026589	770.829091	18.760167	-0.095644	1.601250
515.652352	763.068353	18.765171	-0.095569	1.594256
515.757026	755.186455	18.770176	-0.095583	1.587190
515.641485	747.347199	18.775181	-0.095556	1.580100
515.323871	739.561729	18.780186	-0.095492	1.572997
515.277362	731.699944	18.785191	-0.095478	1.565832
515.341492	723.874930	18.790195	-0.095485	1.558684
515.313022	716.009144	18.795200	-0.095475	1.551452
515.323350	708.166264	18.800205	-0.095472	1.544213
515.328922	700.334978	18.805210	-0.095467	1.536950
515.367542	692.477591	18.810215	-0.095470	1.529633
515.154955	684.700407	18.815219	-0.095425	1.522318
515.007196	676.889288	18.820224	-0.095392	1.514946
515.042184	669.066846	18.825229	-0.095394	1.507554
514.931737	661.253958	18.830234	-0.095368	1.500113
514.712077	653.476543	18.835239	-0.095322	1.492652
514.832869	645.630173	18.840243	-0.095339	1.485140
514.530506	637.873764	18.845248	-0.095278	1.477610
514.555146	630.028637	18.850253	-0.095277	1.470007
514.116993	622.280702	18.855258	-0.095191	1.462386
514.213776	614.437888	18.860263	-0.095204	1.454717
514.474740	606.588442	18.865267	-0.095247	1.447029
513.997358	598.866058	18.870272	-0.095153	1.439304
514.136323	591.052097	18.875277	-0.095174	1.431548
514.241619	583.232103	18.880282	-0.095188	1.423738
514.100672	575.465824	18.885287	-0.095157	1.415897
514.153232	567.682566	18.890291	-0.095162	1.408029
514.163995	559.895109	18.895296	-0.095159	1.400105
513.936379	552.175219	18.900301	-0.095111	1.392164
513.653243	544.419419	18.905306	-0.095053	1.384131
513.595162	536.645423	18.910311	-0.095038	1.376072
513.294071	528.929617	18.915315	-0.094976	1.367983
512.758495	521.246551	18.920320	-0.094872	1.359839
512.842104	513.455015	18.925325	-0.094882	1.351641
512.894549	505.674760	18.930330	-0.094887	1.343399
512.886744	497.907999	18.935335	-0.094880	1.335110
512.432205	490.245715	18.940339	-0.094791	1.326801
512.128195	482.540710	18.945344	-0.094729	1.318420
512.601783	474.631962	18.950349	-0.094812	1.309906
512.597771	466.859122	18.955354	-0.094806	1.301397
512.387689	459.174534	18.960359	-0.094762	1.292892
512.485602	451.427726	18.965363	-0.094775	1.284319
512.413768	443.720759	18.970368	-0.094757	1.275701
512.150565	436.063592	18.975373	-0.094703	1.267043
512.239850	428.326806	18.980378	-0.094714	1.258304
511.640022	420.722689	18.985383	-0.094598	1.249521
511.729009	413.011199	18.990387	-0.094609	1.240687
511.500273	405.356524	18.995392	-0.094562	1.231793
511.499319	397.653164	19.000397	-0.094556	1.222823
511.355722	389.985360	19.005402	-0.094525	1.213799
510.872486	382.378645	19.010407	-0.094430	1.204712
511.024818	374.682694	19.015411	-0.094453	1.195578
510.855634	367.034926	19.020416	-0.094416	1.186366
510.688262	359.408049	19.025421	-0.094380	1.177107
510.183575	351.837021	19.030426	-0.094281	1.167773
510.066520	344.190853	19.035431	-0.094255	1.158353
510.203307	336.505123	19.040435	-0.094275	1.148860
509.938589	328.891531	19.045440	-0.094221	1.139292
509.359879	321.361643	19.050445	-0.094108	1.129680
508.769196	313.839219	19.055450	-0.093993	1.119993
507.830998	306.367534	19.060455	-0.093814	1.110209
507.347522	298.814012	19.065459	-0.093719	1.100333
505.350962	291.507752	19.070464	-0.093342	1.090350
501.233253	284.538171	19.075469	-0.092571	1.080235
498.438402	277.284783	19.080474	-0.092046	1.069948
496.729512	269.824907	19.085479	-0.091722	1.059534
494.848970	262.410263	19.090483	-0.091367	1.049038
493.025123	254.980118	19.095488	-0.091023	1.038426
491.529505	247.515287	19.100493	-0.090740	1.027735
490.209304	240.022768	19.105498	-0.090489	1.016935
488.657166	232.583416	19.110503	-0.090195	1.006036
487.463563	225.118476	19.115507	-0.089968	0.995070
486.105331	217.653130	19.120512	-0.089710	0.983939
484.789443	210.230757	19.125517	-0.089460	0.972754
483.679972	202.785689	19.130522	-0.089249	0.961458
482.522927	195.369827	19.135527	-0.089028	0.950058
481.509141	187.952217	19.140531	-0.088835	0.938555
480.176053	180.608637	19.145536	-0.088582	0.926936
479.092051	173.266900	19.150541	-0.088375	0.915240
477.977811	165.927124	19.155546	-0.088163	0.903387
476.456838	158.685338	19.160551	-0.087875	0.891418
475.680526	151.339107	19.165555	-0.087726	0.879329
474.717087	144.042941	19.170560	-0.087541	0.867099
473.814206	136.780435	19.175565	-0.087369	0.854767
472.758028	129.573259	19.180570	-0.087167	0.842302
471.362212	122.441866	19.185575	-0.086903	0.829677
470.328815	115.268055	19.190579	-0.086706	0.816893
469.410044	108.099247	19.195584	-0.086530	0.803951
468.422629	100.991539	19.200589	-0.086341	0.790884
467.127411	93.965705	19.205594	-0.086095	0.777648
465.778044	86.976794	19.210599	-0.085840	0.764233
465.033146	79.921658	19.215603	-0.085696	0.750656
463.894294	73.146566	19.220608	-0.085480	0.737235