Mon Apr 19 08:51:00 2021

Number of Points = 3635
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.962194	-0.013912	0.000000	-0.000008	0.309512

2.586899	0.057488	0.005005	0.000062	0.309527
3.003031	-0.021212	0.010010	-0.000015	0.309513
3.100634	-0.037535	0.015014	-0.000034	0.309519
2.816187	0.015455	0.020019	0.000019	0.309525
2.413196	0.088168	0.025024	0.000094	0.309522
2.700062	0.038268	0.030029	0.000041	0.309533
2.806809	0.016176	0.035034	0.000021	0.309520
2.762936	0.024097	0.040038	0.000030	0.309519
2.509742	0.071734	0.045043	0.000077	0.309527
2.647424	0.045567	0.050048	0.000051	0.309521
2.469480	0.079962	0.055053	0.000084	0.309531
2.224216	0.124452	0.060058	0.000130	0.309530
2.348531	0.103572	0.065062	0.000107	0.309538
2.700855	0.036654	0.070067	0.000041	0.309524
2.096588	0.148757	0.075072	0.000154	0.309535
2.876054	-0.037447	0.080077	0.000009	0.309326
2.906004	-0.062423	0.085082	0.000003	0.309235
2.354090	0.041581	0.090086	0.000106	0.309252
2.689585	-0.020622	0.095091	0.000044	0.309246
2.851572	-0.052381	0.100096	0.000014	0.309235
2.602867	-0.005088	0.105101	0.000060	0.309244
1.881411	0.126792	0.110106	0.000194	0.309248
2.057136	0.069888	0.115110	0.000162	0.309131
2.218675	-0.005947	0.120115	0.000132	0.308913
1.931443	0.045381	0.125120	0.000185	0.308909
2.327974	-0.026336	0.130125	0.000111	0.308910
2.700171	-0.097544	0.135130	0.000042	0.308893
2.158324	0.004516	0.140134	0.000143	0.308910
1.478671	0.103452	0.145139	0.000269	0.308795
2.222159	-0.073140	0.150144	0.000131	0.308600
2.002591	-0.031045	0.155149	0.000172	0.308610
1.969982	-0.026544	0.160154	0.000178	0.308603
2.448819	-0.116434	0.165158	0.000089	0.308589
2.598505	-0.187052	0.170163	0.000061	0.308386
2.180576	-0.135689	0.175168	0.000139	0.308270
2.230856	-0.143552	0.180173	0.000130	0.308276
2.410423	-0.177414	0.185178	0.000096	0.308270
2.179569	-0.183611	0.190182	0.000140	0.308044
1.691384	-0.106292	0.195187	0.000230	0.307990
2.020495	-0.167324	0.200192	0.000169	0.307984
2.562837	-0.272183	0.205197	0.000068	0.307954
1.890812	-0.215615	0.210202	0.000193	0.307646
2.160921	-0.264436	0.215206	0.000143	0.307647
2.268031	-0.283363	0.220211	0.000123	0.307649
2.148328	-0.315483	0.225216	0.000146	0.307396
1.645770	-0.233222	0.230221	0.000239	0.307353
1.935369	-0.289154	0.235226	0.000185	0.307337
1.864152	-0.319127	0.240230	0.000199	0.307135
2.004887	-0.371840	0.245235	0.000173	0.307007
1.865859	-0.346397	0.250240	0.000199	0.307007
2.388834	-0.484980	0.255245	0.000101	0.306802
1.580207	-0.354182	0.260250	0.000252	0.306725
2.329242	-0.495185	0.265254	0.000112	0.306702
2.323361	-0.563436	0.270259	0.000114	0.306375
1.986135	-0.502223	0.275264	0.000176	0.306374
1.895925	-0.515512	0.280269	0.000193	0.306234
2.067935	-0.581457	0.285274	0.000161	0.306070
1.897332	-0.552571	0.290278	0.000193	0.306060
1.633321	-0.567364	0.295283	0.000242	0.305763
1.709875	-0.582062	0.300288	0.000228	0.305759
1.822372	-0.633859	0.305293	0.000207	0.305610
1.835051	-0.660636	0.310298	0.000205	0.305494
1.885454	-0.694509	0.315302	0.000196	0.305377
2.036196	-0.767383	0.320307	0.000168	0.305161
1.994993	-0.775998	0.325312	0.000175	0.305084
1.814601	-0.792626	0.330317	0.000209	0.304850
2.021846	-0.841113	0.335322	0.000171	0.304798
1.812836	-0.862810	0.340326	0.000210	0.304514
1.607649	-0.829599	0.345331	0.000248	0.304495
1.584996	-0.881568	0.350336	0.000252	0.304228
1.548161	-0.874722	0.355341	0.000259	0.304229
1.133501	-0.868545	0.360346	0.000336	0.303899
0.710072	-0.789441	0.365350	0.000415	0.303909
1.197797	-0.935245	0.370355	0.000324	0.303637
1.131302	-0.933213	0.375360	0.000337	0.303589
1.115797	-0.987834	0.380365	0.000340	0.303315
0.419411	-0.866720	0.385370	0.000469	0.303289
0.807850	-0.988199	0.390374	0.000397	0.303045
0.920830	-1.020866	0.395379	0.000376	0.302987
0.770457	-1.055183	0.400384	0.000404	0.302693
1.012398	-1.106390	0.405389	0.000359	0.302658
0.752983	-1.126281	0.410394	0.000408	0.302337
0.470418	-1.079294	0.415398	0.000460	0.302316
0.703258	-1.183997	0.420403	0.000417	0.302017
0.787890	-1.217864	0.425408	0.000401	0.301928
0.746741	-1.254951	0.430413	0.000409	0.301714
0.869684	-1.316130	0.435418	0.000386	0.301528
1.009883	-1.376292	0.440422	0.000360	0.301361
0.900853	-1.405698	0.445427	0.000381	0.301125
0.526310	-1.356342	0.450432	0.000450	0.301034
0.786342	-1.460349	0.455437	0.000402	0.300761
0.181110	-1.370157	0.460442	0.000515	0.300666
-0.180438	-1.330489	0.465446	0.000582	0.300540
0.288633	-1.464880	0.470451	0.000495	0.300303
-0.011122	-1.434094	0.475456	0.000551	0.300189
0.111786	-1.522413	0.480461	0.000528	0.299871
0.189977	-1.563051	0.485466	0.000513	0.299743
0.057386	-1.578704	0.490470	0.000538	0.299551
-0.041944	-1.604312	0.495475	0.000557	0.299340
-0.507341	-1.542525	0.500480	0.000643	0.299229
-0.120052	-1.676000	0.505485	0.000571	0.298924
0.144863	-1.762127	0.510490	0.000522	0.298740
-0.096393	-1.747380	0.515494	0.000567	0.298599
-0.172981	-1.795801	0.520499	0.000581	0.298296
-0.612957	-1.740326	0.525504	0.000663	0.298177
-0.447122	-1.804795	0.530509	0.000633	0.298010
-0.843921	-1.794707	0.535514	0.000706	0.297709
-0.826210	-1.825876	0.540518	0.000703	0.297573
-0.795891	-1.875519	0.545523	0.000698	0.297358
-1.172779	-1.859862	0.550528	0.000768	0.297100
-1.165858	-1.888452	0.555533	0.000767	0.296967
-1.185183	-1.931266	0.560538	0.000770	0.296741
-1.532829	-1.909586	0.565542	0.000835	0.296538
-1.158295	-2.010215	0.570547	0.000765	0.296379
-1.108970	-2.076847	0.575552	0.000756	0.296097
-1.152003	-2.108848	0.580557	0.000764	0.295902
-0.920535	-2.189786	0.585562	0.000721	0.295712
-1.422102	-2.136485	0.590566	0.000815	0.295527
-2.421605	-2.001643	0.595571	0.001001	0.295297
-2.421627	-2.033696	0.600576	0.001001	0.295140
-2.392146	-2.091158	0.605581	0.000996	0.294884
-2.305426	-2.150929	0.610586	0.000979	0.294668
-2.349960	-2.175288	0.615590	0.000988	0.294508
-2.749817	-2.154188	0.620595	0.001062	0.294254
-3.356680	-2.080608	0.625600	0.001175	0.294074
-3.279165	-2.124718	0.630605	0.001161	0.293926
-3.390969	-2.166080	0.635610	0.001182	0.293621
-3.424702	-2.188621	0.640614	0.001188	0.293480
-3.924366	-2.134470	0.645619	0.001281	0.293299
-4.314149	-2.109682	0.650624	0.001354	0.293071
-4.653871	-2.063379	0.655629	0.001417	0.292995
-5.441540	-1.982901	0.660634	0.001564	0.292685
-4.439520	-2.187742	0.665638	0.001377	0.292572
-4.880288	-2.152888	0.670643	0.001459	0.292348
-5.581241	-2.061057	0.675648	0.001590	0.292172
-5.061264	-2.187078	0.680653	0.001493	0.292015
-5.091514	-2.233399	0.685658	0.001499	0.291758
-5.514025	-2.177233	0.690662	0.001578	0.291656
-5.633704	-2.210207	0.695667	0.001600	0.291384
-5.316716	-2.299564	0.700672	0.001541	0.291226
-5.780534	-2.245238	0.705677	0.001627	0.291077
-6.494780	-2.163667	0.710682	0.001760	0.290837
-6.588607	-2.161512	0.715686	0.001778	0.290762
-6.704081	-2.185320	0.720691	0.001799	0.290539
-6.986686	-2.149472	0.725696	0.001852	0.290461
-7.362505	-2.138232	0.730701	0.001922	0.290177
-6.865178	-2.250667	0.735706	0.001830	0.290067
-7.603538	-2.159944	0.740710	0.001967	0.289849
-7.346457	-2.234881	0.745715	0.001919	0.289708
-7.695228	-2.211637	0.750720	0.001984	0.289507
-7.957992	-2.195254	0.755725	0.002033	0.289350
-8.390011	-2.141441	0.760730	0.002114	0.289226
-8.463161	-2.170813	0.765734	0.002127	0.289012
-8.587111	-2.168237	0.770739	0.002150	0.288912
-8.836796	-2.172367	0.775744	0.002197	0.288664
-8.718731	-2.211421	0.780749	0.002175	0.288576
-8.651323	-2.272190	0.785754	0.002163	0.288332
-9.184683	-2.190315	0.790758	0.002262	0.288256
-9.230938	-2.227970	0.795763	0.002271	0.288024
-9.293331	-2.230417	0.800768	0.002282	0.287955
-9.503911	-2.246726	0.805773	0.002322	0.287680
-10.327836	-2.105253	0.810778	0.002475	0.287638
-10.105528	-2.198490	0.815782	0.002434	0.287372
-10.512253	-2.133135	0.820787	0.002509	0.287329
-10.541756	-2.175988	0.825792	0.002515	0.287085
-10.692324	-2.166008	0.830797	0.002543	0.286998
-10.675444	-2.202765	0.835802	0.002540	0.286827
-11.273009	-2.117535	0.840806	0.002651	0.286709
-11.274480	-2.145367	0.845811	0.002651	0.286567
-11.883305	-2.072578	0.850816	0.002765	0.286375
-11.478244	-2.156447	0.855821	0.002689	0.286323
-12.292713	-2.057485	0.860826	0.002841	0.286075
-11.943848	-2.122581	0.865830	0.002776	0.286066
-12.058338	-2.154347	0.870835	0.002798	0.285800
-12.563195	-2.070291	0.875840	0.002892	0.285760
-12.802760	-2.052316	0.880845	0.002936	0.285631
-12.489374	-2.133963	0.885850	0.002878	0.285505
-12.752100	-2.106202	0.890854	0.002927	0.285404
-13.163908	-2.078047	0.895859	0.003004	0.285166
-13.158278	-2.078395	0.900864	0.003003	0.285170
-13.245138	-2.120609	0.905869	0.003019	0.284875
-13.544670	-2.072735	0.910874	0.003075	0.284841
-13.773686	-2.065190	0.915878	0.003117	0.284668
-13.068723	-2.224786	0.920883	0.002986	0.284508
-13.962512	-2.073995	0.925888	0.003153	0.284448
-13.727497	-2.161824	0.930893	0.003109	0.284218
-13.959642	-2.117212	0.935898	0.003152	0.284230
-14.419432	-2.094871	0.940902	0.003238	0.283918
-14.524427	-2.079587	0.945907	0.003257	0.283898
-14.576794	-2.099998	0.950912	0.003267	0.283745
-14.118936	-2.217805	0.955917	0.003182	0.283569
-14.749306	-2.112346	0.960922	0.003299	0.283522
-15.751216	-1.978426	0.965926	0.003486	0.283275
-15.412762	-2.038406	0.970931	0.003423	0.283283
-15.559010	-2.049773	0.975936	0.003450	0.283089
-15.805329	-2.024001	0.980941	0.003496	0.282991
-15.305972	-2.123041	0.985946	0.003403	0.282949
-15.794609	-2.096332	0.990950	0.003494	0.282631
-15.979092	-2.061300	0.995955	0.003529	0.282638
-16.486442	-2.002401	1.000960	0.003623	0.282467
-16.119335	-2.095972	1.005965	0.003555	0.282329
-16.435962	-2.040397	1.010970	0.003614	0.282319
-17.156519	-1.970781	1.015974	0.003748	0.282004
-16.578653	-2.075357	1.020979	0.003641	0.282006
-16.729856	-2.072900	1.025984	0.003669	0.281877
-16.987602	-2.058764	1.030989	0.003717	0.281709
-17.016115	-2.053285	1.035994	0.003722	0.281710
-17.089733	-2.094972	1.040998	0.003736	0.281427
-17.957503	-1.941761	1.046003	0.003897	0.281403
-17.686614	-2.003965	1.051008	0.003847	0.281336
-17.373436	-2.110335	1.056013	0.003789	0.281082
-17.752385	-2.043141	1.061018	0.003859	0.281073
-18.123297	-2.015058	1.066022	0.003928	0.280870
-18.004920	-2.057046	1.071027	0.003907	0.280764
-18.355953	-1.994059	1.076032	0.003972	0.280760
-17.891678	-2.126115	1.081037	0.003886	0.280514
-17.935009	-2.119829	1.086042	0.003894	0.280505
-17.928207	-2.159136	1.091046	0.003892	0.280308
-18.327864	-2.114888	1.096051	0.003967	0.280161
-18.539756	-2.083934	1.101056	0.004006	0.280122
-18.541970	-2.135342	1.106061	0.004007	0.279854
-18.296338	-2.182002	1.111066	0.003961	0.279843
-18.833343	-2.132871	1.116070	0.004061	0.279592
-19.050069	-2.103717	1.121075	0.004102	0.279539
-19.048531	-2.122999	1.126080	0.004101	0.279440
-19.220745	-2.133576	1.131085	0.004133	0.279223
-19.162985	-2.143537	1.136090	0.004123	0.279225
-19.185932	-2.195670	1.141094	0.004127	0.278933
-19.248491	-2.193419	1.146099	0.004139	0.278886
-19.504664	-2.176038	1.151104	0.004187	0.278734
-19.611042	-2.186352	1.156109	0.004206	0.278579
-19.962931	-2.127333	1.161114	0.004272	0.278553
-20.481844	-2.088314	1.166118	0.004369	0.278265
-20.430396	-2.095123	1.171123	0.004359	0.278279
-20.290784	-2.156285	1.176128	0.004333	0.278092
-21.032830	-2.041734	1.181133	0.004471	0.277986
-20.629425	-2.116296	1.186138	0.004396	0.277979
-20.765555	-2.157332	1.191142	0.004422	0.277636
-20.977772	-2.117848	1.196147	0.004461	0.277641
-21.306092	-2.088096	1.201152	0.004522	0.277484
-21.366794	-2.107557	1.206157	0.004534	0.277325
-21.007583	-2.173905	1.211162	0.004467	0.277319
-21.511222	-2.146046	1.216166	0.004561	0.276986
-21.462994	-2.151609	1.221171	0.004552	0.277003
-22.061178	-2.068825	1.226176	0.004663	0.276867
-22.505864	-2.015109	1.231181	0.004746	0.276724
-22.335484	-2.047487	1.236186	0.004714	0.276717
-22.196368	-2.123945	1.241190	0.004688	0.276449
-22.372673	-2.105244	1.246195	0.004721	0.276379
-22.327550	-2.129305	1.251200	0.004713	0.276295
-22.081716	-2.220706	1.256205	0.004667	0.276050
-22.155413	-2.206321	1.261210	0.004681	0.276055
-23.089363	-2.087649	1.266214	0.004855	0.275787
-22.708352	-2.164099	1.271219	0.004784	0.275749
-22.633885	-2.196112	1.276224	0.004770	0.275652
-22.923193	-2.172869	1.281229	0.004824	0.275497
-23.034941	-2.151488	1.286234	0.004845	0.275503
-22.975367	-2.225123	1.291238	0.004834	0.275172
-23.021629	-2.219713	1.296243	0.004843	0.275156
-23.297359	-2.204107	1.301248	0.004894	0.274974
-23.465565	-2.199446	1.306253	0.004925	0.274837
-23.417558	-2.218654	1.311258	0.004916	0.274782
-24.145609	-2.139199	1.316262	0.005052	0.274503
-24.101373	-2.143877	1.321267	0.005044	0.274520
-24.211662	-2.159703	1.326272	0.005064	0.274331
-24.823681	-2.065070	1.331277	0.005178	0.274242
-24.532194	-2.125145	1.336282	0.005124	0.274205
-24.613749	-2.169198	1.341286	0.005139	0.273894
-24.575501	-2.175349	1.346291	0.005132	0.273898
-25.258840	-2.086073	1.351296	0.005260	0.273712
-25.251057	-2.111950	1.356301	0.005258	0.273583
-24.992920	-2.159087	1.361306	0.005210	0.273582
-25.377931	-2.150517	1.366310	0.005282	0.273256
-25.049460	-2.210209	1.371315	0.005221	0.273256
-24.986830	-2.253220	1.376320	0.005209	0.273088
-25.537588	-2.174295	1.381325	0.005312	0.272975
-25.437435	-2.202503	1.386330	0.005293	0.272922
-25.811041	-2.188961	1.391334	0.005363	0.272633
-25.347939	-2.272415	1.396339	0.005277	0.272637
-26.033716	-2.195504	1.401344	0.005404	0.272383
-26.774616	-2.071744	1.406349	0.005542	0.272324
-26.517267	-2.125923	1.411354	0.005494	0.272285
-26.744169	-2.140185	1.416358	0.005537	0.271989
-27.194144	-2.053587	1.421363	0.005620	0.272014
-26.916432	-2.131876	1.426368	0.005569	0.271866
-27.427196	-2.065099	1.431373	0.005664	0.271727
-27.183108	-2.112416	1.436378	0.005619	0.271711
-27.643306	-2.080158	1.441382	0.005704	0.271436
-27.542587	-2.107100	1.446387	0.005686	0.271390
-27.480696	-2.131355	1.451392	0.005674	0.271321
-27.665776	-2.145073	1.456397	0.005709	0.271067
-27.678369	-2.140670	1.461402	0.005711	0.271078
-28.006331	-2.119818	1.466406	0.005772	0.270871
-27.880723	-2.165668	1.471411	0.005749	0.270748
-27.585627	-2.227660	1.476416	0.005694	0.270703
-27.904781	-2.209890	1.481421	0.005753	0.270487
-28.467396	-2.104435	1.486426	0.005858	0.270504
-28.487374	-2.142074	1.491430	0.005862	0.270283
-28.137365	-2.230803	1.496435	0.005797	0.270148
-28.458380	-2.183035	1.501440	0.005857	0.270091
-28.784635	-2.174477	1.506445	0.005917	0.269818
-28.402568	-2.243632	1.511450	0.005846	0.269820
-28.762589	-2.224732	1.516454	0.005913	0.269570
-28.976559	-2.199127	1.521459	0.005953	0.269498
-28.909075	-2.229170	1.526464	0.005941	0.269402
-29.566206	-2.142545	1.531469	0.006063	0.269225
-29.528915	-2.150262	1.536474	0.006056	0.269220
-29.627813	-2.184890	1.541478	0.006075	0.268936
-29.466711	-2.225602	1.546483	0.006045	0.268875
-29.874277	-2.170718	1.551488	0.006121	0.268771
-29.986628	-2.188818	1.556493	0.006142	0.268563
-29.769969	-2.226808	1.561498	0.006101	0.268570
-30.170090	-2.208726	1.566502	0.006176	0.268275
-30.318105	-2.187037	1.571507	0.006204	0.268247
-30.359776	-2.202156	1.576512	0.006211	0.268124
-30.481085	-2.211236	1.581517	0.006234	0.267955
-30.436074	-2.220013	1.586522	0.006226	0.267952
-30.889681	-2.199641	1.591526	0.006310	0.267616
-30.636762	-2.245607	1.596531	0.006263	0.267616
-31.112595	-2.190705	1.601536	0.006352	0.267444
-31.473412	-2.152143	1.606541	0.006419	0.267297
-31.234468	-2.194609	1.611546	0.006374	0.267303
-31.632910	-2.182981	1.616550	0.006449	0.266973
-31.564388	-2.193316	1.621555	0.006436	0.266984
-31.553998	-2.223050	1.626560	0.006434	0.266833
-31.765066	-2.210509	1.631565	0.006473	0.266692
-31.906380	-2.186906	1.636570	0.006500	0.266680
-32.277091	-2.180906	1.641574	0.006569	0.266346
-32.170834	-2.197605	1.646579	0.006549	0.266361
-32.330816	-2.199999	1.651584	0.006579	0.266189
-32.359002	-2.222460	1.656589	0.006584	0.266039
-32.290054	-2.238265	1.661594	0.006571	0.266021
-32.438371	-2.266983	1.666598	0.006599	0.265717
-32.716293	-2.214405	1.671603	0.006651	0.265728
-33.019882	-2.192115	1.676608	0.006707	0.265548
-32.901744	-2.229419	1.681613	0.006686	0.265462
-33.240218	-2.176451	1.686618	0.006749	0.265415
-33.780791	-2.131524	1.691622	0.006849	0.265123
-33.148187	-2.246350	1.696627	0.006732	0.265124
-33.786536	-2.168606	1.701632	0.006850	0.264914
-34.092617	-2.132178	1.706637	0.006907	0.264809
-33.666835	-2.215685	1.711642	0.006828	0.264775
-34.129016	-2.185471	1.716646	0.006914	0.264480
-34.112096	-2.187214	1.721651	0.006911	0.264487
-34.017628	-2.237628	1.726656	0.006894	0.264305
-34.005857	-2.261522	1.731661	0.006892	0.264186
-33.991129	-2.278720	1.736666	0.006889	0.264106
-34.998255	-2.142020	1.741670	0.007076	0.263851
-34.618605	-2.209365	1.746675	0.007006	0.263860
-34.801133	-2.216573	1.751680	0.007040	0.263638
-35.086059	-2.182027	1.756685	0.007093	0.263542
-35.113039	-2.187783	1.761690	0.007098	0.263484
-35.388487	-2.185461	1.766694	0.007149	0.263221
-35.152723	-2.227062	1.771699	0.007105	0.263227
-35.545122	-2.194238	1.776704	0.007179	0.263015
-35.681932	-2.183125	1.781709	0.007204	0.262939
-35.402872	-2.249989	1.786714	0.007152	0.262850
-36.323669	-2.130045	1.791718	0.007324	0.262588
-35.907569	-2.203359	1.796723	0.007246	0.262601
-36.276307	-2.173514	1.801728	0.007315	0.262395
-36.848464	-2.086746	1.806733	0.007421	0.262299
-36.672503	-2.119634	1.811738	0.007389	0.262294
-36.651919	-2.183673	1.816742	0.007385	0.261961
-36.716743	-2.172493	1.821747	0.007397	0.261957
-37.158140	-2.113306	1.826752	0.007479	0.261840
-37.287702	-2.118386	1.831757	0.007503	0.261681
-36.961252	-2.176998	1.836762	0.007443	0.261685
-37.627420	-2.107814	1.841766	0.007567	0.261397
-37.557047	-2.128628	1.846771	0.007554	0.261353
-37.228538	-2.202790	1.851776	0.007493	0.261273
-37.726881	-2.155690	1.856781	0.007585	0.261031
-37.783544	-2.144501	1.861786	0.007596	0.261035
-37.707317	-2.198737	1.866790	0.007582	0.260811
-37.843997	-2.191042	1.871795	0.007607	0.260716
-38.103188	-2.151528	1.876800	0.007656	0.260673
-37.908537	-2.224545	1.881805	0.007619	0.260464
-37.861577	-2.231071	1.886810	0.007611	0.260475
-38.501045	-2.162892	1.891814	0.007730	0.260207
-38.371482	-2.200862	1.896819	0.007706	0.260126
-38.175361	-2.252457	1.901824	0.007669	0.260037
-38.609872	-2.216375	1.906829	0.007750	0.259798
-38.465533	-2.241157	1.911834	0.007723	0.259806
-38.751135	-2.243798	1.916838	0.007777	0.259501
-39.013984	-2.199514	1.921843	0.007826	0.259481
-39.379481	-2.156124	1.926848	0.007894	0.259352
-39.641479	-2.134185	1.931853	0.007943	0.259208
-38.964304	-2.258663	1.936858	0.007817	0.259200
-39.896068	-2.148967	1.941862	0.007990	0.258866
-40.022094	-2.125820	1.946867	0.008014	0.258867
-39.872432	-2.174551	1.951872	0.007986	0.258746
-40.264987	-2.136344	1.956877	0.008059	0.258560
-40.284650	-2.131479	1.961882	0.008063	0.258567
-40.886406	-2.068789	1.966886	0.008175	0.258305
-40.536507	-2.142718	1.971891	0.008110	0.258247
-40.736063	-2.114749	1.976896	0.008147	0.258200
-40.818880	-2.144283	1.981901	0.008162	0.257949
-40.561580	-2.190115	1.986906	0.008114	0.257954
-40.953790	-2.160523	1.991910	0.008187	0.257720
-41.183141	-2.139552	1.996915	0.008230	0.257603
-40.979084	-2.209586	2.001920	0.008192	0.257417

-41.600443	-2.126109	2.011917	0.008308	0.257250
-41.899500	-2.120377	2.021914	0.008364	0.256976
-41.903434	-2.141627	2.031910	0.008365	0.256852
-41.996871	-2.155062	2.041907	0.008382	0.256679
-42.258235	-2.137769	2.051904	0.008431	0.256508
-42.701143	-2.084929	2.061901	0.008513	0.256351
-42.705073	-2.082651	2.071898	0.008514	0.256359
-42.823696	-2.099213	2.081894	0.008536	0.256143
-43.352158	-2.018521	2.091891	0.008635	0.256055
-43.210868	-2.044421	2.101888	0.008609	0.256054
-43.609505	-1.970478	2.111885	0.008683	0.256061
-42.872240	-2.106934	2.121882	0.008546	0.256048
-42.882370	-2.105868	2.131878	0.008548	0.256043
-43.378224	-2.012739	2.141875	0.008640	0.256059
-43.365268	-2.014023	2.151872	0.008638	0.256065
-43.314390	-2.023988	2.161869	0.008628	0.256060
-43.720911	-1.945986	2.171866	0.008704	0.256082
-43.279877	-2.029823	2.181862	0.008622	0.256062
-43.118540	-2.061277	2.191859	0.008592	0.256049
-43.328111	-2.020759	2.201856	0.008631	0.256062
-43.060706	-2.070875	2.211853	0.008582	0.256054
-42.708103	-2.101272	2.221850	0.008516	0.256244
-42.832116	-2.057763	2.231846	0.008539	0.256362
-42.944812	-2.036399	2.241843	0.008560	0.256366
-43.457230	-1.939779	2.251840	0.008656	0.256385
-43.317845	-1.916179	2.261837	0.008630	0.256661
-42.891780	-1.984012	2.271834	0.008550	0.256715
-42.712874	-2.013584	2.281830	0.008517	0.256731
-42.241273	-2.054553	2.291827	0.008430	0.256984
-42.359951	-2.032682	2.301824	0.008452	0.256985
-42.224166	-2.037274	2.311821	0.008427	0.257098
-41.702690	-2.095315	2.321818	0.008330	0.257305
-41.824900	-2.072610	2.331814	0.008352	0.257307
-41.501572	-2.087855	2.341811	0.008292	0.257552
-41.686321	-2.041819	2.351808	0.008327	0.257621
-41.476834	-2.051418	2.361805	0.008288	0.257781
-41.394683	-2.032484	2.371802	0.008273	0.257971
-41.172810	-2.052622	2.381798	0.008231	0.258084
-40.782646	-2.095256	2.391795	0.008159	0.258242
-40.899261	-2.053989	2.401792	0.008181	0.258354
-40.320585	-2.122069	2.411789	0.008073	0.258562
-40.348746	-2.097588	2.421786	0.008078	0.258670
-40.331484	-2.062622	2.431782	0.008075	0.258883
-40.146232	-2.065283	2.441779	0.008041	0.259056
-40.167958	-2.031959	2.451776	0.008045	0.259220
-39.877855	-2.046768	2.461773	0.007991	0.259432
-39.409112	-2.119739	2.471770	0.007904	0.259500
-39.809337	-1.987418	2.481766	0.007978	0.259831
-39.456903	-2.028614	2.491763	0.007913	0.259959
-39.207388	-2.040082	2.501760	0.007866	0.260147
-38.944239	-2.038694	2.511757	0.007818	0.260421
-39.300168	-1.944662	2.521754	0.007884	0.260583
-38.691920	-2.027404	2.531750	0.007771	0.260738
-38.158233	-2.081742	2.541747	0.007671	0.260974
-38.111342	-2.071122	2.551744	0.007663	0.261080
-37.670080	-2.103131	2.561741	0.007581	0.261347
-37.409552	-2.117145	2.571738	0.007532	0.261532
-37.268884	-2.116286	2.581734	0.007506	0.261678
-37.073460	-2.101508	2.591731	0.007470	0.261956
-37.234032	-2.043635	2.601728	0.007500	0.262114
-36.462123	-2.150644	2.611725	0.007356	0.262298
-36.745802	-2.048499	2.621722	0.007409	0.262576
-36.512789	-2.054960	2.631718	0.007366	0.262774
-36.698163	-1.979481	2.641715	0.007400	0.263003
-36.169112	-2.031053	2.651712	0.007302	0.263249
-35.767990	-2.062453	2.661709	0.007227	0.263477
-35.484106	-2.082037	2.671706	0.007175	0.263653
-34.962508	-2.137712	2.681702	0.007078	0.263867
-34.640570	-2.150322	2.691699	0.007018	0.264119
-34.729252	-2.106010	2.701696	0.007034	0.264273
-34.376713	-2.130221	2.711693	0.006969	0.264491
-34.178446	-2.118382	2.721690	0.006932	0.264753
-34.023327	-2.114937	2.731686	0.006903	0.264926
-33.685084	-2.139134	2.741683	0.006840	0.265129
-33.558075	-2.105150	2.751680	0.006817	0.265440
-33.118772	-2.158066	2.761677	0.006735	0.265587
-32.998072	-2.152738	2.771674	0.006713	0.265735
-32.419979	-2.201369	2.781670	0.006605	0.266043
-32.231409	-2.206920	2.791667	0.006570	0.266199
-32.360651	-2.151645	2.801664	0.006594	0.266371
-32.182076	-2.124176	2.811661	0.006561	0.266696
-32.291586	-2.067516	2.821658	0.006581	0.266895
-32.126977	-2.054995	2.831654	0.006551	0.267125
-32.126514	-2.009442	2.841651	0.006551	0.267372
-31.381150	-2.098364	2.851648	0.006412	0.267624
-31.158757	-2.085013	2.861645	0.006371	0.267915
-31.038194	-2.070785	2.871642	0.006348	0.268110
-30.564948	-2.120755	2.881638	0.006260	0.268304
-30.304713	-2.118653	2.891635	0.006212	0.268570
-29.649562	-2.194714	2.901632	0.006090	0.268802
-29.608146	-2.166644	2.911629	0.006083	0.268993
-29.054380	-2.227225	2.921626	0.005980	0.269209
-29.346204	-2.124130	2.931622	0.006034	0.269477
-29.188836	-2.112930	2.941619	0.006005	0.269691
-28.822837	-2.143672	2.951616	0.005937	0.269883
-28.700403	-2.115969	2.961613	0.005914	0.270150
-28.638884	-2.068959	2.971610	0.005903	0.270461
-27.889442	-2.170585	2.981606	0.005763	0.270647
-27.871493	-2.143603	2.991603	0.005760	0.270808
-27.515630	-2.160987	3.001600	0.005694	0.271060
-27.382482	-2.135357	3.011597	0.005669	0.271326
-27.000119	-2.166740	3.021594	0.005598	0.271529
-26.997125	-2.123164	3.031590	0.005597	0.271764
-27.159295	-2.047975	3.041587	0.005628	0.272007
-26.607070	-2.092562	3.051584	0.005525	0.272304
-26.690938	-2.032552	3.061581	0.005541	0.272541
-25.858351	-2.142510	3.071578	0.005386	0.272761
-25.768647	-2.114768	3.081574	0.005369	0.272994
-25.648691	-2.085437	3.091571	0.005347	0.273265
-25.152104	-2.127166	3.101568	0.005254	0.273522
-25.114062	-2.094445	3.111565	0.005247	0.273731
-24.521317	-2.163005	3.121562	0.005137	0.273938
-24.256580	-2.157997	3.131558	0.005088	0.274218
-24.147102	-2.133788	3.141555	0.005068	0.274451
-24.000956	-2.118505	3.151552	0.005041	0.274671
-23.655001	-2.140143	3.161549	0.004976	0.274888
-23.332718	-2.148068	3.171546	0.004916	0.275154
-22.935833	-2.168188	3.181542	0.004842	0.275428
-23.168154	-2.090211	3.191539	0.004886	0.275615
-23.023677	-2.078636	3.201536	0.004859	0.275813
-22.896662	-2.052832	3.211533	0.004835	0.276069
-22.543625	-2.059189	3.221530	0.004770	0.276372
-22.002096	-2.112203	3.231526	0.004669	0.276610
-21.902759	-2.089080	3.241523	0.004651	0.276825
-21.783588	-2.067692	3.251520	0.004628	0.277049
-21.332094	-2.098905	3.261517	0.004544	0.277315
-20.940418	-2.116412	3.271514	0.004472	0.277595
-20.651010	-2.123846	3.281510	0.004418	0.277830
-20.348917	-2.140944	3.291507	0.004362	0.278027
-19.714289	-2.215100	3.301504	0.004244	0.278241
-20.092513	-2.091741	3.311501	0.004314	0.278524
-19.676070	-2.125429	3.321498	0.004237	0.278742
-19.615686	-2.091345	3.331494	0.004225	0.278976
-19.225116	-2.115315	3.341491	0.004153	0.279219
-18.889116	-2.123511	3.351488	0.004090	0.279493
-18.497718	-2.156392	3.361485	0.004018	0.279691
-18.367887	-2.137595	3.371482	0.003994	0.279910
-18.557710	-2.053742	3.381478	0.004029	0.280164
-18.427581	-2.009837	3.391475	0.004005	0.280513
-18.224505	-2.010702	3.401472	0.003967	0.280698
-18.133256	-1.982060	3.411469	0.003950	0.280931
-17.687226	-2.011381	3.421466	0.003867	0.281197
-17.911582	-1.917547	3.431462	0.003909	0.281470
-17.799672	-1.881807	3.441459	0.003888	0.281758
-16.938863	-1.991692	3.451456	0.003728	0.281997
-16.434034	-2.026360	3.461453	0.003634	0.282289
-15.705444	-2.116385	3.471450	0.003499	0.282507
-15.544999	-2.106681	3.481446	0.003469	0.282705
-15.320690	-2.098507	3.491443	0.003427	0.282955
-15.204965	-2.066044	3.501440	0.003406	0.283229
-14.683034	-2.121914	3.511437	0.003309	0.283428
-14.780231	-2.059118	3.521434	0.003327	0.283658
-14.712746	-2.026698	3.531430	0.003314	0.283885
-13.852794	-2.119237	3.541427	0.003154	0.284210
-13.804110	-2.094574	3.551424	0.003145	0.284380
-13.696944	-2.073698	3.561421	0.003125	0.284585
-13.252786	-2.107757	3.571418	0.003043	0.284822
-13.120386	-2.071719	3.581414	0.003018	0.285127
-12.862172	-2.071300	3.591411	0.002970	0.285367
-12.710219	-2.059612	3.601408	0.002942	0.285566
-12.147327	-2.127901	3.611405	0.002837	0.285738
-12.006283	-2.094973	3.621402	0.002811	0.286034
-11.698190	-2.113832	3.631398	0.002754	0.286221
-11.492585	-2.111996	3.641395	0.002716	0.286419
-11.349828	-2.084185	3.651392	0.002689	0.286690
-11.057873	-2.086437	3.661389	0.002635	0.286946
-11.039140	-2.044524	3.671386	0.002631	0.287174
-10.701550	-2.063253	3.681382	0.002569	0.287389
-10.415509	-2.066969	3.691379	0.002515	0.287632
-10.289605	-2.027994	3.701376	0.002492	0.287942
-10.185523	-2.003967	3.711373	0.002473	0.288158
-10.028581	-1.985554	3.721370	0.002444	0.288393
-9.589298	-2.020689	3.731366	0.002362	0.288617
-9.292060	-2.018373	3.741363	0.002307	0.288899
-9.427912	-1.936053	3.751360	0.002332	0.289187
-8.721402	-2.020743	3.761357	0.002201	0.289405
-8.847408	-1.950443	3.771354	0.002224	0.289642
-8.783886	-1.909086	3.781350	0.002212	0.289906
-8.190582	-1.963752	3.791347	0.002102	0.290171
-7.957036	-1.944453	3.801344	0.002058	0.290478
-7.495998	-1.991392	3.811341	0.001973	0.290661
-7.367137	-1.972273	3.821338	0.001949	0.290873
-7.066510	-1.982685	3.831334	0.001893	0.291092
-6.795531	-1.972608	3.841331	0.001843	0.291387
-6.958498	-1.889126	3.851328	0.001873	0.291654
-6.576828	-1.910815	3.861325	0.001802	0.291890
-6.395990	-1.896712	3.871322	0.001768	0.292122
-5.946748	-1.930061	3.881318	0.001685	0.292361
-5.925520	-1.876814	3.891315	0.001681	0.292643
-6.096338	-1.781668	3.901312	0.001713	0.292960
-5.338706	-1.870714	3.911309	0.001572	0.293199
-5.279402	-1.831935	3.921306	0.001561	0.293444
-5.313310	-1.770183	3.931302	0.001567	0.293717
-4.885802	-1.794936	3.941299	0.001488	0.293978
-4.563287	-1.799946	3.951296	0.001428	0.294241
-4.133357	-1.819834	3.961293	0.001348	0.294527
-4.223384	-1.749053	3.971290	0.001365	0.294794
-4.045328	-1.726109	3.981286	0.001332	0.295065
-3.363402	-1.794354	3.991283	0.001205	0.295337
-3.576337	-1.703518	4.001280	0.001244	0.295592
-2.739101	-1.815028	4.011277	0.001089	0.295791
-2.572386	-1.786831	4.021274	0.001058	0.296077
-2.648124	-1.718584	4.031270	0.001072	0.296342
-2.701863	-1.646810	4.041267	0.001082	0.296644
-2.666001	-1.601957	4.051264	0.001075	0.296895
-2.626251	-1.547509	4.061261	0.001068	0.297195
-2.334867	-1.541383	4.071258	0.001014	0.297482
-2.235275	-1.492662	4.081254	0.000995	0.297806
-2.051805	-1.462176	4.091251	0.000961	0.298116
-2.132761	-1.387304	4.101248	0.000976	0.298407
-1.842031	-1.372060	4.111245	0.000922	0.298737
-1.880083	-1.296595	4.121242	0.000929	0.299068
-1.582355	-1.285450	4.131238	0.000874	0.299383
-1.625661	-1.210833	4.141235	0.000882	0.299705
-1.617261	-1.138658	4.151232	0.000880	0.300061
-1.139716	-1.150150	4.161229	0.000792	0.300423
-1.275354	-1.065233	4.171226	0.000817	0.300713
-1.384653	-0.965883	4.181222	0.000837	0.301095
-1.216174	-0.917850	4.191219	0.000806	0.301472
-0.791315	-0.922279	4.201216	0.000727	0.301821
-0.521692	-0.900440	4.211213	0.000677	0.302160
-0.502494	-0.827637	4.221210	0.000673	0.302525
-0.399376	-0.762434	4.231206	0.000654	0.302925
-0.247052	-0.704968	4.241203	0.000626	0.303331
-0.300939	-0.615316	4.251200	0.000636	0.303712
-0.049945	-0.576478	4.261197	0.000589	0.304113
-0.458412	-0.414446	4.271194	0.000665	0.304531
0.165896	-0.438706	4.281190	0.000549	0.304954
0.218605	-0.362922	4.291187	0.000539	0.305358
0.096251	-0.256783	4.301184	0.000562	0.305755
0.209145	-0.180841	4.311181	0.000541	0.306211
0.083327	-0.067542	4.321178	0.000565	0.306637
0.325591	-0.009687	4.331174	0.000519	0.307117
-0.424013	0.224873	4.341171	0.000659	0.307580
0.000000	0.262213	4.351168	0.000580	0.308117

-0.143965	0.556563	4.356173	0.000607	0.309374
0.566700	0.981710	4.361178	0.000474	0.311955
1.221770	1.706845	4.366182	0.000352	0.315846
2.034964	2.690744	4.371187	0.000200	0.320988
2.948732	3.952309	4.376192	0.000029	0.327359
4.229617	5.449370	4.381197	-0.000211	0.334916
6.406805	7.089200	4.386202	-0.000617	0.343594
9.170608	8.951153	4.391206	-0.001133	0.353405
12.950352	10.956415	4.396211	-0.001838	0.364253
18.298773	13.031374	4.401216	-0.002835	0.376150
23.674403	15.474145	4.406221	-0.003838	0.389066
28.564854	18.386397	4.411226	-0.004750	0.402936
32.808609	21.793609	4.416230	-0.005542	0.417651
37.175246	25.569803	4.421235	-0.006358	0.433169
43.424563	29.390394	4.426240	-0.007524	0.449387
50.051296	33.569236	4.431245	-0.008761	0.466358
55.269432	38.415599	4.436250	-0.009735	0.483964
63.578807	43.106643	4.441254	-0.011285	0.502105
74.477322	47.785535	4.446259	-0.013318	0.520869
107.598518	48.959755	4.451264	-0.019486	0.540298
143.799018	50.433895	4.456269	-0.026227	0.561222
144.971280	58.723431	4.461274	-0.026451	0.582652
146.243984	67.271993	4.466278	-0.026693	0.603981
148.290058	75.952867	4.471283	-0.027080	0.625207
150.053170	84.942676	4.476288	-0.027414	0.646309
152.433675	94.051398	4.481293	-0.027863	0.667238
154.766230	103.367656	4.486298	-0.028303	0.687945
158.544852	112.580189	4.491302	-0.029013	0.708358
162.584946	121.968550	4.496307	-0.029771	0.728635
165.335164	131.731652	4.501312	-0.030290	0.748639
169.785977	141.282424	4.506317	-0.031125	0.768288
176.939655	150.516088	4.511322	-0.032463	0.787739
184.714641	159.768270	4.516326	-0.033916	0.806944
192.352642	169.205805	4.521331	-0.035345	0.825977
201.454348	178.466260	4.526336	-0.037045	0.844713
215.811221	186.958231	4.531341	-0.039724	0.863297
223.948462	196.693997	4.536346	-0.041246	0.881720
234.713562	206.030133	4.541350	-0.043256	0.899858
242.098800	216.018470	4.546355	-0.044638	0.917722
254.347125	225.192044	4.551360	-0.046924	0.935295
260.297372	235.502884	4.556365	-0.048039	0.952588
266.402437	245.713248	4.561370	-0.049182	0.969459
274.981623	255.465892	4.566374	-0.050786	0.985998
281.297301	265.585040	4.571379	-0.051969	1.002218
285.756392	275.925819	4.576384	-0.052806	1.018032
290.439620	286.106592	4.581389	-0.053684	1.033433
294.015845	296.367309	4.586394	-0.054357	1.048450
296.780910	306.637528	4.591398	-0.054878	1.063076
300.251810	316.653721	4.596403	-0.055531	1.077326
303.766752	326.526628	4.601408	-0.056192	1.091209
307.108546	336.325757	4.606413	-0.056820	1.104780
310.113555	346.081507	4.611418	-0.057386	1.118054
313.329114	355.681784	4.616422	-0.057991	1.131019
315.794091	365.334387	4.621427	-0.058456	1.143739
319.314369	374.693334	4.626432	-0.059118	1.156178
322.072623	384.065288	4.631437	-0.059638	1.168338
325.682789	393.229297	4.636442	-0.060316	1.180295
329.312262	402.326109	4.641446	-0.060997	1.192053
332.453688	411.452417	4.646451	-0.061588	1.203630
335.453477	420.528981	4.651456	-0.062153	1.215008
337.396113	429.724372	4.656461	-0.062520	1.226208
340.408573	438.646216	4.661466	-0.063087	1.237198
342.664067	447.610697	4.666470	-0.063513	1.247992
344.562226	456.609465	4.671475	-0.063872	1.258662
346.026730	465.598766	4.676480	-0.064151	1.269148
347.771461	474.458349	4.681485	-0.064481	1.279455
349.993803	483.193930	4.686490	-0.064901	1.289630
351.310661	492.039136	4.691494	-0.065152	1.299677
352.897428	500.820234	4.696499	-0.065453	1.309626
354.744889	509.520891	4.701504	-0.065802	1.319460
356.205610	518.184058	4.706509	-0.066080	1.329109
358.124045	526.719173	4.711514	-0.066443	1.338633
359.600783	535.304909	4.716518	-0.066723	1.348064
360.637588	543.945723	4.721523	-0.066922	1.357409
361.591953	552.547394	4.726528	-0.067105	1.366635
362.483067	561.129363	4.731533	-0.067277	1.375766
364.064002	569.555793	4.736538	-0.067576	1.384795
364.280584	578.220880	4.741542	-0.067622	1.393777
365.332123	586.656613	4.746547	-0.067824	1.402609
366.938179	594.986931	4.751552	-0.068128	1.411371
367.991433	603.404367	4.756557	-0.068330	1.420074
369.043714	611.830284	4.761562	-0.068531	1.428731
370.154242	620.209025	4.766566	-0.068743	1.437299
371.289886	628.567609	4.771571	-0.068960	1.445800
372.546911	636.917503	4.776576	-0.069199	1.454261
373.871672	645.233791	4.781581	-0.069452	1.462651
375.478337	653.539660	4.786586	-0.069756	1.471028
376.765036	661.847291	4.791590	-0.070001	1.479307
378.135929	670.134577	4.796595	-0.070262	1.487534
379.370576	678.448292	4.801600	-0.070497	1.495719
380.470801	686.769161	4.806605	-0.070707	1.503844
381.455946	695.132451	4.811610	-0.070896	1.511948
382.770989	703.373322	4.816614	-0.071146	1.519943
384.231716	711.608168	4.821619	-0.071423	1.527913
385.059106	719.952951	4.826624	-0.071583	1.535847
386.514763	728.169366	4.831629	-0.071859	1.543716
387.376261	736.529842	4.836634	-0.072025	1.551588
388.406295	744.784848	4.841638	-0.072222	1.559349
388.955689	753.146411	4.846643	-0.072330	1.567096
389.788502	761.438778	4.851648	-0.072490	1.574785
390.596213	769.695095	4.856653	-0.072646	1.582399
391.576714	777.940630	4.861658	-0.072834	1.589992
392.179725	786.230318	4.866662	-0.072952	1.597533
394.248300	794.234652	4.871667	-0.073342	1.604995
395.504076	802.469963	4.876672	-0.073581	1.612510
396.426939	810.715658	4.881677	-0.073758	1.619952
397.300126	819.000192	4.886682	-0.073926	1.627387
398.326656	827.230934	4.891686	-0.074123	1.634762
399.658054	835.372472	4.896691	-0.074376	1.642069
400.721384	843.575897	4.901696	-0.074579	1.649359
401.157165	851.897177	4.906701	-0.074666	1.656632
402.140038	860.093453	4.911706	-0.074854	1.663840
402.725060	868.350676	4.916710	-0.074968	1.671015
403.296412	876.606389	4.921715	-0.075080	1.678156
404.127939	884.772227	4.926720	-0.075240	1.685225
404.590734	893.032779	4.931725	-0.075332	1.692295
404.998438	901.292137	4.936730	-0.075413	1.699327
405.654021	909.464494	4.941734	-0.075540	1.706290
406.407215	917.660238	4.946739	-0.075686	1.713257
406.770085	925.869750	4.951744	-0.075759	1.720155
407.183626	934.070793	4.956749	-0.075841	1.727026
407.760482	942.273068	4.961754	-0.075954	1.733891
408.339314	950.420164	4.966758	-0.076067	1.740684
409.286604	958.543301	4.971763	-0.076248	1.747478
410.188932	966.682959	4.976768	-0.076422	1.754253
411.300446	974.757662	4.981773	-0.076634	1.760975
411.629985	983.028833	4.986778	-0.076701	1.767732
412.362340	991.190510	4.991782	-0.076842	1.774426
413.108683	999.330153	4.996787	-0.076986	1.781077
413.915858	1007.500110	5.001792	-0.077142	1.787736
415.215221	1015.580132	5.006797	-0.077389	1.794359
415.413658	1023.830481	5.011802	-0.077431	1.800957
415.990331	1031.965449	5.016806	-0.077544	1.807486
416.384815	1040.184704	5.021811	-0.077623	1.814035
416.863800	1048.355541	5.026816	-0.077717	1.820533
417.329499	1056.512310	5.031821	-0.077809	1.826995
418.551178	1064.556746	5.036826	-0.078042	1.833437
419.343826	1072.663002	5.041830	-0.078195	1.839853
419.490604	1080.897209	5.046835	-0.078227	1.846269
420.256201	1089.022418	5.051840	-0.078375	1.852652
421.083749	1097.127580	5.056845	-0.078535	1.859004
421.339933	1105.338987	5.061850	-0.078588	1.865349
421.773028	1113.507090	5.066854	-0.078674	1.871660
421.842649	1121.727171	5.071859	-0.078692	1.877946
422.421437	1129.826784	5.076864	-0.078805	1.884180
422.713098	1137.969274	5.081869	-0.078864	1.890391
423.377554	1146.076545	5.086874	-0.078993	1.896599
423.605748	1154.231024	5.091878	-0.079041	1.902772
424.495119	1162.292545	5.096883	-0.079212	1.908930
424.527492	1170.503465	5.101888	-0.079223	1.915083
425.130351	1178.597131	5.106893	-0.079341	1.921193
425.834440	1186.690896	5.111898	-0.079477	1.927295
426.361378	1194.814087	5.116902	-0.079580	1.933380
426.851095	1202.942533	5.121907	-0.079677	1.939444
427.579968	1211.021212	5.126912	-0.079818	1.945480
427.498530	1219.256174	5.131917	-0.079808	1.951522
427.767808	1227.401427	5.136922	-0.079863	1.957519
428.456095	1235.429239	5.141926	-0.079997	1.963457
428.659763	1243.599619	5.146931	-0.080040	1.969428
429.155078	1251.708307	5.151936	-0.080137	1.975368
429.551041	1259.804188	5.156941	-0.080216	1.981270
430.197946	1267.903173	5.161946	-0.080342	1.987183
430.112157	1276.101428	5.166950	-0.080331	1.993072
430.660380	1284.161137	5.171955	-0.080439	1.998911
430.938727	1292.275365	5.176960	-0.080496	2.004744
431.359970	1300.378905	5.181965	-0.080579	2.010567
431.578438	1308.535251	5.186970	-0.080625	2.016389
432.277269	1316.566909	5.191974	-0.080761	2.022157
432.291060	1324.742327	5.196979	-0.080769	2.027938
432.986721	1332.811440	5.201984	-0.080903	2.033699
432.952606	1340.968862	5.206989	-0.080902	2.039429
434.157399	1348.904904	5.211994	-0.081132	2.045116
434.529371	1357.036292	5.216998	-0.081206	2.050838
434.615604	1365.218296	5.222003	-0.081228	2.056550
435.216723	1373.277733	5.227008	-0.081345	2.062214
435.368219	1381.421579	5.232013	-0.081378	2.067874
435.654029	1389.559202	5.237018	-0.081437	2.073529
435.637983	1397.703946	5.242022	-0.081439	2.079142
436.349705	1405.705051	5.247027	-0.081577	2.084715
437.252091	1413.745976	5.252032	-0.081750	2.090319
437.537809	1421.849947	5.257037	-0.081808	2.095889
437.986985	1429.959781	5.262042	-0.081897	2.101465
438.309975	1438.081095	5.267046	-0.081963	2.107021
439.077497	1446.150307	5.272051	-0.082111	2.112571
439.519350	1454.263957	5.277056	-0.082198	2.118104
439.960450	1462.323094	5.282061	-0.082286	2.123586
439.548533	1470.561708	5.287066	-0.082214	2.129092
440.021297	1478.616434	5.292070	-0.082307	2.134546
440.087471	1486.743371	5.297075	-0.082325	2.139994
440.137975	1494.863856	5.302080	-0.082340	2.145424
440.912666	1502.860999	5.307085	-0.082489	2.150826
441.071439	1510.984223	5.312090	-0.082524	2.156240
441.227575	1519.074624	5.317094	-0.082558	2.161618
441.434027	1527.168431	5.322099	-0.082602	2.166990
442.055189	1535.212212	5.327104	-0.082723	2.172355
442.538929	1543.267188	5.332109	-0.082818	2.177700
442.461769	1551.424963	5.337114	-0.082809	2.183048
442.962106	1559.498481	5.342118	-0.082907	2.188381
443.493217	1567.529573	5.347123	-0.083011	2.193676
443.714670	1575.633688	5.352128	-0.083058	2.198977
443.917648	1583.701966	5.357133	-0.083101	2.204240
444.251584	1591.817229	5.362138	-0.083168	2.209534
444.510845	1599.905248	5.367142	-0.083222	2.214790
444.836353	1607.981075	5.372147	-0.083288	2.220031
445.246528	1616.043214	5.377152	-0.083369	2.225259
445.183850	1624.202717	5.382157	-0.083363	2.230495
445.290669	1632.304181	5.387162	-0.083388	2.235696
445.522315	1640.355300	5.392166	-0.083436	2.240865
446.230714	1648.340377	5.397171	-0.083573	2.246022
446.451404	1656.445593	5.402176	-0.083620	2.251199
447.081526	1664.467004	5.407181	-0.083742	2.256348
447.323903	1672.581186	5.412186	-0.083793	2.261510
447.453200	1680.705092	5.417190	-0.083822	2.266656
447.567977	1688.845618	5.422195	-0.083849	2.271799
448.157883	1696.882663	5.427200	-0.083964	2.276908
448.161865	1704.956346	5.432205	-0.083970	2.281976
448.330108	1713.031018	5.437210	-0.084006	2.287049
448.819965	1721.059832	5.442214	-0.084102	2.292109
449.142997	1729.131753	5.447219	-0.084168	2.297170
449.718535	1737.156807	5.452224	-0.084280	2.302213
449.771400	1745.276519	5.457229	-0.084295	2.307259
450.310987	1753.333605	5.462234	-0.084401	2.312296
450.344730	1761.437552	5.467238	-0.084412	2.317308
450.655613	1769.462360	5.472243	-0.084476	2.322284
451.125443	1777.524515	5.477248	-0.084568	2.327286
451.163910	1785.655858	5.482253	-0.084581	2.332283
451.450870	1793.734342	5.487258	-0.084639	2.337257
451.549849	1801.822615	5.492262	-0.084663	2.342212
451.918287	1809.870981	5.497267	-0.084737	2.347154
452.233625	1817.955584	5.502272	-0.084801	2.352103
451.593055	1826.139940	5.507277	-0.084687	2.357024
451.837622	1834.174802	5.512282	-0.084737	2.361916
452.474291	1842.144589	5.517286	-0.084861	2.366791
453.382882	1850.104126	5.522291	-0.085036	2.371672
453.110638	1858.295286	5.527296	-0.084990	2.376586
453.722317	1866.264255	5.532301	-0.085109	2.381428
453.459185	1874.441599	5.537306	-0.085065	2.386315
453.826439	1882.498791	5.542310	-0.085139	2.391170
453.852790	1890.588743	5.547315	-0.085149	2.396008
454.714525	1898.522293	5.552320	-0.085315	2.400809
454.621279	1906.665219	5.557325	-0.085303	2.405649
454.837660	1914.759001	5.562330	-0.085348	2.410475
455.468289	1922.747843	5.567334	-0.085471	2.415262
455.495153	1930.841170	5.572339	-0.085481	2.420053
455.401747	1938.984790	5.577344	-0.085469	2.424855
455.522745	1947.054573	5.582349	-0.085497	2.429621
455.930566	1955.123301	5.587354	-0.085578	2.434399
456.257699	1963.146436	5.592358	-0.085644	2.439135
456.706210	1971.131764	5.597363	-0.085733	2.443849
456.958462	1979.231351	5.602368	-0.085785	2.448605
456.766941	1987.353064	5.607373	-0.085754	2.453331
457.297884	1995.365076	5.612378	-0.085858	2.458039
457.220370	2003.474252	5.617382	-0.085849	2.462748
458.014726	2011.421945	5.622387	-0.086002	2.467421
458.241374	2019.501305	5.627392	-0.086050	2.472118
458.321613	2027.584499	5.632397	-0.086070	2.476797
458.604471	2035.637389	5.637402	-0.086128	2.481465
458.838229	2043.691408	5.642406	-0.086176	2.486121
459.363072	2051.724465	5.647411	-0.086279	2.490778
459.916943	2059.772400	5.652416	-0.086388	2.495437
459.990072	2067.851137	5.657421	-0.086407	2.500069
459.815486	2075.999666	5.662426	-0.086379	2.504714
459.578160	2084.154626	5.667430	-0.086340	2.509350
459.749520	2092.176863	5.672435	-0.086377	2.513931
459.871680	2100.228986	5.677440	-0.086405	2.518518
459.985465	2108.233900	5.682445	-0.086432	2.523069
460.472489	2116.233806	5.687450	-0.086528	2.527635
460.741254	2124.301086	5.692454	-0.086583	2.532216
460.659000	2132.387414	5.697459	-0.086573	2.536774
461.374899	2140.370366	5.702464	-0.086711	2.541323
461.028533	2148.510936	5.707469	-0.086652	2.545876
461.361514	2156.554771	5.712474	-0.086719	2.550415
462.048073	2164.537193	5.717478	-0.086852	2.554937
462.052376	2172.594090	5.722483	-0.086858	2.559444
461.984175	2180.707419	5.727488	-0.086851	2.563969
462.624269	2188.701576	5.732493	-0.086975	2.568470
462.675060	2196.800156	5.737498	-0.086990	2.572980
462.975339	2204.845745	5.742502	-0.087051	2.577470
463.316109	2212.864946	5.747507	-0.087120	2.581940
463.410771	2220.973850	5.752512	-0.087142	2.586434
463.591528	2229.066027	5.757517	-0.087181	2.590918
463.665910	2237.220819	5.762522	-0.087200	2.595421
463.723473	2245.240699	5.767526	-0.087216	2.599841
463.521590	2253.269218	5.772531	-0.087184	2.604240
463.759864	2261.305460	5.777536	-0.087234	2.608666
463.947895	2269.340382	5.782541	-0.087274	2.613081
464.086600	2277.380873	5.787546	-0.087305	2.617488
464.214971	2285.410252	5.792550	-0.087334	2.621880
464.738357	2293.380345	5.797555	-0.087436	2.626260
465.059241	2301.467263	5.802560	-0.087501	2.630682
464.832724	2309.587713	5.807565	-0.087465	2.635078
465.274517	2317.561229	5.812570	-0.087552	2.639431
465.535446	2325.606854	5.817574	-0.087606	2.643805
465.930045	2333.605856	5.822579	-0.087684	2.648155
466.125603	2341.690792	5.827584	-0.087726	2.652531
466.464221	2349.740898	5.832589	-0.087794	2.656890
466.516563	2357.845341	5.837594	-0.087809	2.661252
466.703683	2365.855850	5.842598	-0.087849	2.665566
466.957609	2373.911506	5.847603	-0.087902	2.669901
467.196807	2381.997972	5.852608	-0.087952	2.674245
467.301666	2390.038085	5.857613	-0.087976	2.678548
467.358791	2398.093488	5.862618	-0.087992	2.682849
467.602800	2406.137995	5.867622	-0.088043	2.687149
468.007449	2414.154916	5.872627	-0.088123	2.691439
468.301930	2422.195263	5.877632	-0.088183	2.695727
468.371823	2430.270423	5.882637	-0.088202	2.700012
468.360989	2438.325693	5.887642	-0.088205	2.704274
468.111659	2446.451964	5.892646	-0.088164	2.708552
468.187595	2454.492019	5.897651	-0.088183	2.712799
468.986902	2462.417548	5.902656	-0.088337	2.717024
469.363284	2470.441626	5.907661	-0.088412	2.721268
469.504564	2478.510157	5.912666	-0.088444	2.725513
469.328470	2486.640597	5.917670	-0.088416	2.729765
469.501938	2494.674481	5.922675	-0.088454	2.733981
469.792899	2502.702700	5.927680	-0.088513	2.738195
470.233194	2510.684997	5.932685	-0.088600	2.742388
470.504997	2518.737544	5.937690	-0.088656	2.746601
470.604927	2526.838597	5.942694	-0.088680	2.750821
470.762358	2534.933327	5.947699	-0.088714	2.755036
471.496603	2542.869421	5.952704	-0.088856	2.759197
471.186372	2550.955539	5.957709	-0.088804	2.763365
471.380997	2559.022676	5.962714	-0.088845	2.767548
471.517350	2567.091436	5.967718	-0.088876	2.771722
471.461758	2575.150112	5.972723	-0.088871	2.775873
471.495150	2583.219511	5.977728	-0.088882	2.780029
471.750994	2591.191117	5.982733	-0.088935	2.784142
471.730257	2599.276344	5.987738	-0.088936	2.788290
472.132246	2607.274965	5.992742	-0.089016	2.792413
472.350083	2615.311950	5.997747	-0.089062	2.796538
472.663529	2623.338210	6.002752	-0.089125	2.800658
472.148665	2631.460872	6.007757	-0.089035	2.804771
473.007963	2639.387061	6.012762	-0.089200	2.808860
473.525174	2647.429920	6.017766	-0.089301	2.812982
473.584142	2655.497752	6.022771	-0.089318	2.817083
473.823518	2663.563383	6.027776	-0.089367	2.821188
473.987680	2671.591563	6.032781	-0.089403	2.825263
474.744121	2679.578287	6.037786	-0.089549	2.829346
475.254969	2687.612541	6.042790	-0.089650	2.833433
474.820172	2695.734003	6.047795	-0.089574	2.837503
474.358793	2703.905295	6.052800	-0.089493	2.841591
474.906774	2711.809641	6.057805	-0.089600	2.845597
475.627726	2719.771085	6.062810	-0.089740	2.849635
476.085331	2727.837704	6.067814	-0.089830	2.853706
476.064092	2735.901758	6.072819	-0.089831	2.857742
476.479890	2743.937110	6.077824	-0.089914	2.861783
476.856823	2751.938384	6.082829	-0.089989	2.865799
476.962541	2760.047493	6.087834	-0.090014	2.869847
477.348171	2768.093924	6.092838	-0.090091	2.873875
477.117801	2776.177745	6.097843	-0.090054	2.877880
477.236498	2784.261230	6.102848	-0.090081	2.881900
477.598484	2792.221688	6.107853	-0.090154	2.885867
478.092999	2800.206878	6.112858	-0.090251	2.889847
478.494220	2808.275070	6.117862	-0.090331	2.893858
478.464002	2816.359727	6.122867	-0.090330	2.897848
478.665963	2824.426521	6.127872	-0.090373	2.901836
478.941238	2832.430394	6.132877	-0.090430	2.905791
479.109701	2840.487035	6.137882	-0.090466	2.909761
479.432260	2848.559363	6.142886	-0.090531	2.913742
478.788324	2856.702516	6.147891	-0.090417	2.917700
479.021754	2864.685635	6.152896	-0.090465	2.921622
479.398878	2872.632492	6.157901	-0.090541	2.925528
479.192834	2880.727184	6.162906	-0.090508	2.929470
479.588688	2888.726944	6.167910	-0.090586	2.933392
480.108338	2896.656724	6.172915	-0.090688	2.937282
480.482228	2904.719215	6.177920	-0.090763	2.941223
481.068838	2912.694913	6.182925	-0.090878	2.945128
481.321529	2920.773913	6.187930	-0.090930	2.949060
481.773243	2928.817054	6.192934	-0.091019	2.952980
481.979881	2936.849936	6.197939	-0.091063	2.956877
482.150268	2944.940784	6.202944	-0.091100	2.960795
482.534775	2952.918937	6.207949	-0.091177	2.964664
483.155637	2960.928902	6.212954	-0.091297	2.968556
482.915683	2969.056072	6.217958	-0.091258	2.972455
482.714002	2977.176674	6.222963	-0.091226	2.976347
483.332967	2985.144880	6.227968	-0.091346	2.980203
483.884405	2993.109468	6.232973	-0.091454	2.984049
483.559897	3001.262481	6.237978	-0.091399	2.987935
483.402861	3009.381930	6.242982	-0.091375	2.991809
483.737342	3017.341691	6.247987	-0.091442	2.995627
484.051179	3025.331016	6.252992	-0.091506	2.999452
484.386369	3033.312704	6.257997	-0.091573	3.003271
484.083367	3041.459050	6.263002	-0.091522	3.007130
483.861354	3049.565054	6.268006	-0.091486	3.010970
484.194474	3057.509436	6.273011	-0.091553	3.014755
484.292309	3065.565256	6.278016	-0.091577	3.018577
484.710068	3073.519139	6.283021	-0.091660	3.022362
485.155657	3081.545733	6.288026	-0.091748	3.026178
485.619439	3089.584102	6.293030	-0.091839	3.029995
486.230652	3097.536595	6.298035	-0.091958	3.033774
486.161229	3105.654644	6.303040	-0.091951	3.037593
486.017127	3113.761431	6.308045	-0.091929	3.041398
486.196003	3121.762235	6.313050	-0.091967	3.045165
486.352518	3129.789350	6.318054	-0.092002	3.048937
486.476296	3137.873231	6.323059	-0.092030	3.052731
486.987497	3145.881776	6.328064	-0.092130	3.056503
487.059905	3153.896979	6.333069	-0.092149	3.060252
487.299241	3161.914228	6.338074	-0.092199	3.064006
487.157733	3170.043590	6.343078	-0.092178	3.067788
487.167182	3178.112411	6.348083	-0.092185	3.071546
486.963285	3186.237161	6.353088	-0.092152	3.075314
487.242961	3194.166302	6.358093	-0.092209	3.079010
487.105800	3202.191427	6.363098	-0.092189	3.082727
487.418769	3210.189091	6.368102	-0.092252	3.086447
487.361395	3218.232871	6.373107	-0.092247	3.090167
487.571764	3226.307814	6.378112	-0.092291	3.093910
488.073572	3234.245401	6.383117	-0.092390	3.097598
488.153061	3242.273332	6.388122	-0.092410	3.101303
488.683606	3250.249134	6.393126	-0.092514	3.105001
489.019704	3258.270597	6.398131	-0.092581	3.108707
489.101014	3266.362087	6.403136	-0.092602	3.112428
489.310638	3274.410279	6.408141	-0.092646	3.116131
489.260024	3282.468990	6.413146	-0.092642	3.119823
489.516418	3290.477900	6.418150	-0.092695	3.123501
489.456974	3298.529244	6.423155	-0.092689	3.127180
489.855813	3306.559492	6.428160	-0.092768	3.130866
490.093638	3314.589381	6.433165	-0.092818	3.134540
490.438280	3322.594924	6.438170	-0.092887	3.138203
491.035878	3330.589785	6.443174	-0.093004	3.141869
490.869975	3338.697842	6.448179	-0.092978	3.145547
490.931668	3346.765369	6.453184	-0.092995	3.149213
491.430301	3354.727048	6.458189	-0.093093	3.152846
491.459796	3362.786961	6.463194	-0.093103	3.156498
491.772957	3370.804977	6.468198	-0.093167	3.160140
491.890191	3378.782439	6.473203	-0.093194	3.163751
491.956989	3386.903399	6.478208	-0.093211	3.167420
492.307632	3394.900881	6.483213	-0.093282	3.171041
492.388936	3402.919292	6.488218	-0.093302	3.174656
492.791291	3410.962977	6.493222	-0.093382	3.178292
492.705955	3419.016699	6.498227	-0.093372	3.181908
492.648675	3427.093539	6.503232	-0.093366	3.185530
492.437554	3435.171385	6.508237	-0.093332	3.189143
493.369190	3443.059096	6.513242	-0.093511	3.192715
493.794296	3451.114370	6.518246	-0.093595	3.196337
493.862557	3459.146764	6.523251	-0.093613	3.199929
494.371470	3467.120204	6.528256	-0.093713	3.203509
494.535969	3475.201547	6.533261	-0.093749	3.207119
494.947900	3483.203990	6.538266	-0.093831	3.210700
495.291470	3491.261403	6.543270	-0.093900	3.214298
495.150956	3499.331030	6.548275	-0.093879	3.217877
495.266141	3507.414949	6.553280	-0.093906	3.221470
495.580646	3515.393305	6.558285	-0.093969	3.225020
495.327751	3523.520138	6.563290	-0.093927	3.228608
495.554143	3531.538089	6.568294	-0.093975	3.232164
495.881296	3539.495440	6.573299	-0.094041	3.235694
496.570109	3547.417873	6.578304	-0.094174	3.239219
496.682322	3555.482517	6.583309	-0.094200	3.242779
496.537883	3563.550935	6.588314	-0.094179	3.246326
496.725787	3571.622042	6.593318	-0.094219	3.249884
497.118037	3579.603503	6.598323	-0.094297	3.253407
497.043159	3587.678374	6.603328	-0.094288	3.256948
497.158593	3595.705935	6.608333	-0.094315	3.260473
496.604256	3603.804045	6.613338	-0.094217	3.263997
496.687860	3611.869041	6.618342	-0.094238	3.267529
496.620428	3619.897366	6.623347	-0.094230	3.271035
496.986520	3627.867341	6.628352	-0.094304	3.274529
497.813254	3635.755880	6.633357	-0.094463	3.278003
497.573427	3643.861707	6.638362	-0.094423	3.281524
497.676133	3651.873145	6.643366	-0.094448	3.285015
498.193926	3659.839620	6.648371	-0.094549	3.288498
498.283905	3667.954315	6.653376	-0.094571	3.292025
498.675478	3675.964773	6.658381	-0.094649	3.295515
498.819966	3683.999748	6.663386	-0.094681	3.299003
499.263525	3692.007691	6.668390	-0.094769	3.302486
498.888741	3700.108736	6.673395	-0.094705	3.305974
499.112151	3708.125435	6.678400	-0.094751	3.309446
499.289113	3716.193919	6.683405	-0.094790	3.312934
499.226076	3724.238812	6.688410	-0.094783	3.316399
500.020362	3732.131517	6.693414	-0.094936	3.319828
500.091632	3740.172609	6.698419	-0.094955	3.323289
500.356101	3748.194802	6.703424	-0.095009	3.326746
500.126587	3756.303423	6.708429	-0.094971	3.330218
500.201590	3764.355612	6.713434	-0.094991	3.333674
500.500500	3772.373122	6.718438	-0.095051	3.337119
501.044647	3780.295003	6.723443	-0.095158	3.340529
500.638634	3788.426302	6.728448	-0.095088	3.343990
501.028998	3796.437565	6.733453	-0.095165	3.347425
501.507940	3804.426080	6.738458	-0.095260	3.350850
500.741314	3812.607842	6.743462	-0.095122	3.354308
501.332789	3820.480685	6.748467	-0.095238	3.357682
501.533285	3828.546980	6.753472	-0.095280	3.361119
501.747112	3836.532250	6.758477	-0.095325	3.364520
501.849303	3844.555961	6.763482	-0.095349	3.367928
501.875735	3852.682802	6.768486	-0.095359	3.371375
502.053954	3860.661842	6.773491	-0.095398	3.374761
502.634884	3868.628451	6.778496	-0.095511	3.378152
502.769918	3876.685135	6.783501	-0.095541	3.381563
502.830786	3884.718630	6.788506	-0.095558	3.384957
503.472973	3892.758809	6.793510	-0.095683	3.388371
503.345756	3900.832073	6.798515	-0.095664	3.391769
503.564780	3908.889195	6.803520	-0.095710	3.395168
503.615069	3916.906396	6.808525	-0.095725	3.398542
504.057425	3924.853872	6.813530	-0.095812	3.401896
504.002535	3932.906379	6.818534	-0.095807	3.405274
504.321336	3940.884790	6.823539	-0.095872	3.408630
504.587279	3948.965142	6.828544	-0.095927	3.412024
504.885493	3956.956919	6.833549	-0.095987	3.415379
504.935522	3964.988626	6.838554	-0.096002	3.418738
504.949472	3973.073900	6.843558	-0.096010	3.422115
504.848108	3981.110872	6.848563	-0.095996	3.425465
505.260443	3989.087610	6.853568	-0.096078	3.428804
505.269283	3997.135697	6.858573	-0.096085	3.432155
505.855667	4005.116232	6.863578	-0.096199	3.435495
506.429037	4013.102130	6.868582	-0.096311	3.438834
506.401287	4021.125108	6.873587	-0.096311	3.442163
506.350220	4029.223277	6.878592	-0.096307	3.445521
506.526485	4037.266274	6.883597	-0.096345	3.448859
506.590320	4045.275767	6.888602	-0.096362	3.452177
506.728186	4053.346647	6.893606	-0.096393	3.455519
506.970835	4061.315607	6.898611	-0.096443	3.458820
506.959980	4069.377140	6.903616	-0.096446	3.462147
507.302176	4077.392927	6.908621	-0.096515	3.465464
507.494250	4085.395291	6.913626	-0.096556	3.468767
507.804521	4093.460392	6.918630	-0.096619	3.472097
507.719259	4101.492923	6.923635	-0.096608	3.475397
507.803143	4109.522572	6.928640	-0.096629	3.478698
507.606290	4117.595987	6.933645	-0.096598	3.482005
507.930145	4125.522812	6.938650	-0.096663	3.485265
508.129006	4133.592193	6.943654	-0.096705	3.488577
508.436609	4141.566087	6.948659	-0.096768	3.491850
508.849648	4149.611100	6.953664	-0.096850	3.495153
508.794861	4157.634251	6.958669	-0.096845	3.498428
508.616630	4165.716702	6.963674	-0.096817	3.501720
508.845516	4173.725733	6.968678	-0.096865	3.504993
509.062709	4181.737142	6.973683	-0.096910	3.508263
508.936429	4189.812095	6.978688	-0.096892	3.511545
509.563210	4197.747599	6.983693	-0.097014	3.514791
509.852612	4205.742298	6.988698	-0.097073	3.518047
509.848395	4213.868114	6.993702	-0.097077	3.521344
510.511695	4221.744288	6.998707	-0.097206	3.524558
510.370951	4229.895031	7.003712	-0.097185	3.527855
510.376528	4237.977257	7.008717	-0.097191	3.531125
510.116697	4245.989979	7.013722	-0.097148	3.534356
510.757253	4253.972024	7.018726	-0.097273	3.537600
510.931439	4261.980228	7.023731	-0.097310	3.540837
511.353904	4269.921959	7.028736	-0.097394	3.544052
511.981137	4277.968009	7.033741	-0.097516	3.547312
511.783349	4286.084179	7.038746	-0.097484	3.550572
511.472242	4294.255897	7.043750	-0.097432	3.553848
511.712871	4302.188203	7.048755	-0.097482	3.557041
511.841187	4310.203120	7.053760	-0.097511	3.560262
511.463939	4318.244521	7.058765	-0.097446	3.563474
511.546120	4326.236869	7.063770	-0.097466	3.566679
512.277102	4334.177191	7.068774	-0.097607	3.569878
512.373268	4342.215886	7.073779	-0.097631	3.573096
513.132337	4350.185391	7.078784	-0.097777	3.576302
513.375313	4358.210718	7.083789	-0.097827	3.579512
513.354822	4366.270619	7.088794	-0.097829	3.582726
513.425086	4374.344410	7.093798	-0.097847	3.585944
514.031464	4382.241026	7.098803	-0.097965	3.589105
514.066405	4390.391650	7.103808	-0.097977	3.592348
513.958208	4398.464984	7.108813	-0.097962	3.595553
514.209788	4406.382414	7.113818	-0.098014	3.598703
514.633852	4414.451098	7.118822	-0.098098	3.601916
514.586066	4422.450186	7.123827	-0.098094	3.605084
514.609292	4430.489827	7.128832	-0.098104	3.608268
514.652792	4438.605400	7.133837	-0.098117	3.611480
514.673377	4446.576557	7.138842	-0.098126	3.614631
515.082803	4454.575899	7.143846	-0.098208	3.617801
515.081603	4462.648171	7.148851	-0.098213	3.620986
515.022520	4470.626293	7.153856	-0.098207	3.624129
515.700491	4478.622453	7.158861	-0.098338	3.627297
515.537887	4486.671124	7.163866	-0.098313	3.630460
515.926569	4494.714053	7.168870	-0.098391	3.633633
515.940641	4502.749216	7.173875	-0.098399	3.636789
515.976704	4510.729346	7.178880	-0.098410	3.639922
516.390975	4518.721762	7.183885	-0.098493	3.643068
516.675800	4526.721545	7.188890	-0.098551	3.646210
516.860124	4534.782436	7.193894	-0.098591	3.649370
516.888501	4542.847653	7.198899	-0.098601	3.652525
517.159298	4550.873511	7.203904	-0.098657	3.655669
517.391000	4558.856306	7.208909	-0.098705	3.658792
517.196621	4566.926599	7.213914	-0.098674	3.661935
517.272218	4574.958772	7.218918	-0.098693	3.665067
517.776454	4582.921204	7.223923	-0.098792	3.668181
518.051456	4590.943205	7.228928	-0.098849	3.671310
518.505931	4598.931043	7.233933	-0.098938	3.674427
518.555040	4606.971069	7.238938	-0.098953	3.677552
519.407167	4614.970075	7.243942	-0.099117	3.680678
518.786390	4623.068376	7.248947	-0.099006	3.683802
519.106201	4631.087444	7.253952	-0.099071	3.686917
519.528778	4639.117043	7.258957	-0.099155	3.690036
519.539101	4647.145666	7.263962	-0.099162	3.693142
519.794106	4655.222129	7.268966	-0.099215	3.696269
519.902109	4663.187518	7.273971	-0.099240	3.699348
520.167421	4671.208269	7.278976	-0.099295	3.702449
520.283218	4679.252234	7.283981	-0.099321	3.705552
520.593760	4687.239890	7.288986	-0.099384	3.708637
521.015153	4695.278192	7.293990	-0.099468	3.711741
521.043016	4703.355692	7.298995	-0.099478	3.714847
521.022958	4711.366679	7.304000	-0.099480	3.717924
521.499724	4719.377992	7.309005	-0.099574	3.721011
521.264895	4727.358488	7.314010	-0.099535	3.724066
521.511095	4735.405593	7.319014	-0.099586	3.727156
521.434754	4743.449306	7.324019	-0.099577	3.730234
521.487700	4751.470909	7.329024	-0.099592	3.733304
521.334281	4759.545063	7.334029	-0.099569	3.736387
521.679048	4767.440239	7.339034	-0.099638	3.739411
522.249587	4775.471610	7.344038	-0.099750	3.742489
522.342948	4783.458270	7.349043	-0.099772	3.745537
522.575312	4791.521374	7.354048	-0.099821	3.748615
522.558046	4799.648002	7.359053	-0.099823	3.751708
522.950469	4807.550266	7.364058	-0.099901	3.754723
523.071294	4815.594443	7.369062	-0.099929	3.757784
522.747196	4823.675543	7.374067	-0.099873	3.760845
523.238957	4831.609314	7.379072	-0.099970	3.763867
523.254063	4839.738312	7.384077	-0.099978	3.766949
523.335345	4847.718181	7.389082	-0.099998	3.769974
523.371270	4855.782389	7.394086	-0.100010	3.773027
523.413621	4863.807339	7.399091	-0.100023	3.776064
523.685438	4871.736254	7.404096	-0.100079	3.779066
523.424708	4879.886160	7.409101	-0.100036	3.782138
523.143039	4887.895689	7.414106	-0.099989	3.785153
524.020818	4895.840975	7.419110	-0.100157	3.788169
524.333526	4903.868695	7.424115	-0.100221	3.791200
523.967076	4911.983850	7.429120	-0.100158	3.794246
524.206378	4919.965915	7.434125	-0.100207	3.797253
524.519200	4927.930890	7.439130	-0.100271	3.800254
524.697810	4935.962735	7.444134	-0.100309	3.803274
524.887464	4943.952942	7.449139	-0.100350	3.806276
525.008678	4951.961114	7.454144	-0.100377	3.809281
525.330799	4960.038804	7.459149	-0.100443	3.812314
525.556667	4967.996920	7.464154	-0.100490	3.815297
525.989029	4976.030219	7.469158	-0.100576	3.818311
526.215045	4984.095540	7.474163	-0.100623	3.821330
526.277763	4992.079869	7.479168	-0.100640	3.824313
526.420095	5000.162089	7.484173	-0.100671	3.827332
526.934355	5008.105174	7.489178	-0.100772	3.830304
526.855372	5016.229848	7.494182	-0.100763	3.833329
526.803949	5024.235142	7.499187	-0.100758	3.836308
527.096116	5032.173148	7.504192	-0.100818	3.839267
526.862143	5040.313108	7.509197	-0.100780	3.842287
527.221361	5048.211045	7.514202	-0.100852	3.845227
527.381543	5056.313368	7.519206	-0.100887	3.848237
527.386755	5064.365198	7.524211	-0.100893	3.851223
527.758677	5072.286228	7.529216	-0.100967	3.854165
527.973326	5080.321042	7.534221	-0.101012	3.857144
528.324412	5088.326649	7.539226	-0.101083	3.860113
528.273843	5096.387236	7.544230	-0.101079	3.863092
528.405066	5104.410073	7.549235	-0.101108	3.866057
528.379871	5112.436821	7.554240	-0.101109	3.869019
528.470085	5120.574274	7.559245	-0.101131	3.872022
528.703686	5128.598304	7.564250	-0.101180	3.874984
529.049973	5136.568103	7.569254	-0.101249	3.877925
529.312423	5144.538513	7.574259	-0.101303	3.880863
529.320897	5152.526392	7.579264	-0.101310	3.883800
529.379688	5160.584755	7.584269	-0.101326	3.886761
529.866892	5168.488257	7.589274	-0.101422	3.889672
530.504384	5176.552414	7.594278	-0.101546	3.892643
530.433345	5184.592948	7.599283	-0.101538	3.895588
530.440609	5192.582477	7.604288	-0.101544	3.898515
530.433889	5200.705070	7.609293	-0.101548	3.901487
530.775242	5208.587315	7.614298	-0.101617	3.904376
531.016194	5216.697109	7.619302	-0.101667	3.907344
530.931497	5224.732866	7.624307	-0.101657	3.910277
530.976619	5232.759236	7.629312	-0.101670	3.913206
531.051105	5240.824374	7.634317	-0.101689	3.916148
531.063703	5248.771971	7.639322	-0.101697	3.919044
531.801929	5256.738325	7.644326	-0.101839	3.921958
531.697439	5264.800107	7.649331	-0.101825	3.924888
531.275213	5272.892875	7.654336	-0.101752	3.927822
531.909082	5280.869269	7.659341	-0.101875	3.930731
532.264676	5288.874715	7.664346	-0.101946	3.933643
532.322410	5296.950543	7.669350	-0.101962	3.936573
532.224508	5304.926579	7.674355	-0.101949	3.939462
532.704652	5312.930898	7.679360	-0.102044	3.942370
532.649320	5321.020142	7.684365	-0.102039	3.945296
532.865655	5328.977348	7.689370	-0.102084	3.948177
533.224532	5337.032727	7.694374	-0.102156	3.951095
533.304988	5345.053613	7.699379	-0.102176	3.953992
533.682090	5353.006825	7.704384	-0.102252	3.956868
533.847619	5361.048360	7.709389	-0.102288	3.959771
534.048531	5369.070722	7.714394	-0.102330	3.962664
533.868957	5377.117720	7.719398	-0.102302	3.965558
534.482047	5385.072734	7.724403	-0.102421	3.968431
534.907898	5393.109796	7.729408	-0.102506	3.971327
534.553680	5401.173362	7.734413	-0.102445	3.974218
534.342359	5409.248803	7.739418	-0.102411	3.977113
534.753811	5417.238261	7.744422	-0.102493	3.979986
534.823265	5425.243963	7.749427	-0.102511	3.982856
534.915146	5433.219528	7.754432	-0.102533	3.985714
535.470836	5441.226812	7.759437	-0.102642	3.988590
535.485116	5449.322506	7.764442	-0.102650	3.991485
535.703361	5457.287765	7.769446	-0.102695	3.994336
536.019699	5465.296186	7.774451	-0.102760	3.997201
536.444239	5473.273931	7.779456	-0.102844	4.000055
536.649107	5481.303693	7.784461	-0.102887	4.002922
536.744005	5489.330381	7.789466	-0.102910	4.005784
536.555763	5497.428549	7.794470	-0.102880	4.008665
536.884267	5505.463957	7.799475	-0.102947	4.011530
536.808951	5513.424491	7.804480	-0.102938	4.014359
536.984447	5521.507507	7.809485	-0.102976	4.017234
537.190533	5529.458678	7.814490	-0.103019	4.020061
537.388483	5537.488960	7.819494	-0.103061	4.022913
537.125111	5545.540502	7.824499	-0.103017	4.025764
537.494196	5553.568436	7.829504	-0.103091	4.028615
537.603521	5561.694953	7.834509	-0.103117	4.031494
537.710810	5569.654418	7.839514	-0.103142	4.034312
537.516073	5577.722064	7.844518	-0.103111	4.037161
538.362693	5585.587746	7.849523	-0.103274	4.039953
538.434478	5593.631171	7.854528	-0.103292	4.042794
538.532662	5601.677370	7.859533	-0.103316	4.045635
538.209107	5609.722784	7.864538	-0.103261	4.048466
538.563383	5617.745285	7.869542	-0.103332	4.051298
538.775004	5625.731796	7.874547	-0.103376	4.054113
539.314809	5633.726760	7.879552	-0.103482	4.056935
539.247427	5641.800495	7.884557	-0.103475	4.059772
539.337344	5649.768289	7.889562	-0.103497	4.062573
539.387225	5657.782457	7.894566	-0.103511	4.065387
539.243375	5665.877116	7.899571	-0.103489	4.068225
539.544179	5673.862557	7.904576	-0.103551	4.071029
539.920148	5681.854961	7.909581	-0.103626	4.073835
539.996820	5689.924326	7.914586	-0.103645	4.076661
540.173298	5697.891665	7.919590	-0.103683	4.079452
540.444897	5705.942811	7.924595	-0.103739	4.082270
540.696642	5713.887828	7.929600	-0.103791	4.085050
541.370488	5721.909746	7.934605	-0.103922	4.087860
541.264753	5729.968148	7.939610	-0.103907	4.090671
541.295970	5737.985332	7.944614	-0.103918	4.093466
541.207489	5746.069287	7.949619	-0.103907	4.096282
541.526562	5753.999893	7.954624	-0.103972	4.099048
541.505920	5762.102971	7.959629	-0.103973	4.101867
541.408633	5770.052978	7.964634	-0.103960	4.104630
541.515752	5778.135987	7.969638	-0.103985	4.107440
542.040167	5786.096730	7.974643	-0.104088	4.110211
541.964578	5794.135032	7.979648	-0.104079	4.112999
542.390039	5802.163858	7.984653	-0.104163	4.115789
542.220903	5810.162653	7.989658	-0.104137	4.118559
542.562868	5818.169715	7.994662	-0.104206	4.121336
542.890873	5826.153079	7.999667	-0.104272	4.124103
542.617703	5834.279458	8.004672	-0.104227	4.126910
543.069750	5842.227540	8.009677	-0.104316	4.129662
543.742674	5850.168300	8.014682	-0.104446	4.132414
543.768767	5858.257354	8.019686	-0.104456	4.135206
544.367830	5866.222836	8.024691	-0.104573	4.137960
544.522188	5874.267414	8.029696	-0.104607	4.140735
544.656830	5882.316370	8.034701	-0.104637	4.143509
544.717027	5890.317250	8.039706	-0.104654	4.146263
544.661057	5898.364028	8.044710	-0.104649	4.149030
544.754556	5906.416204	8.049715	-0.104671	4.151799
545.062703	5914.339697	8.054720	-0.104734	4.154525
544.917130	5922.477650	8.059725	-0.104712	4.157317
545.166943	5930.435783	8.064730	-0.104763	4.160050
545.740725	5938.408741	8.069734	-0.104875	4.162790
545.799067	5946.475544	8.074739	-0.104892	4.165554
545.900027	5954.507019	8.079744	-0.104916	4.168305
546.343846	5962.560206	8.084749	-0.105003	4.171065
546.249950	5970.574512	8.089754	-0.104991	4.173804
546.307921	5978.612587	8.094758	-0.105007	4.176551
546.497916	5986.610306	8.099763	-0.105048	4.179284
546.604382	5994.625341	8.104768	-0.105073	4.182020
547.131717	6002.559994	8.109773	-0.105176	4.184732
546.780829	6010.675290	8.114778	-0.105116	4.187494
547.225776	6018.675639	8.119782	-0.105204	4.190223
547.053803	6026.796434	8.124787	-0.105177	4.192985
547.019200	6034.786665	8.129792	-0.105176	4.195702
547.351292	6042.724990	8.134797	-0.105243	4.198404
547.844056	6050.716651	8.139802	-0.105340	4.201124
547.872419	6058.680941	8.144806	-0.105350	4.203827
548.094252	6066.773945	8.149811	-0.105397	4.206575
547.861938	6074.754251	8.154816	-0.105359	4.209278
548.000146	6082.877121	8.159821	-0.105390	4.212031
547.826302	6090.843684	8.164826	-0.105362	4.214726
548.631962	6098.810268	8.169830	-0.105517	4.217430
548.972509	6106.818109	8.174835	-0.105586	4.220141
549.043485	6114.808210	8.179840	-0.105604	4.222842
549.443879	6122.843219	8.184845	-0.105684	4.225559
549.623465	6130.925524	8.189850	-0.105723	4.228288
549.828995	6138.930847	8.194854	-0.105766	4.230990
549.880005	6146.936799	8.199859	-0.105781	4.233689
550.172087	6154.959167	8.204864	-0.105841	4.236394
549.788108	6163.037650	8.209869	-0.105774	4.239109
550.299579	6170.998898	8.214874	-0.105875	4.241792
550.401021	6178.967299	8.219878	-0.105899	4.244472
550.443299	6187.042921	8.224883	-0.105912	4.247185
550.069639	6195.077257	8.229888	-0.105847	4.249879
550.035967	6203.175578	8.234893	-0.105846	4.252595
550.274977	6211.106367	8.239898	-0.105896	4.255257
550.736053	6219.079683	8.244902	-0.105987	4.257933
551.012247	6227.120346	8.249907	-0.106044	4.260628
551.015533	6235.108590	8.254912	-0.106049	4.263302
551.684671	6243.128042	8.259917	-0.106179	4.265990
551.672689	6251.137191	8.264922	-0.106182	4.268667
552.197706	6259.180495	8.269926	-0.106285	4.271358
552.141081	6267.219770	8.274931	-0.106280	4.274041
551.817115	6275.292886	8.279936	-0.106225	4.276732
552.150713	6283.205195	8.284941	-0.106292	4.279373
553.070681	6291.178048	8.289946	-0.106468	4.282037
553.259104	6299.145709	8.294950	-0.106509	4.284692
553.273397	6307.267526	8.299955	-0.106516	4.287395
553.427609	6315.294084	8.304960	-0.106550	4.290065
553.535250	6323.377670	8.309965	-0.106576	4.292752
553.846074	6331.374617	8.314970	-0.106639	4.295411
553.790333	6339.355943	8.319974	-0.106633	4.298060
554.140729	6347.439170	8.324979	-0.106704	4.300744
553.906341	6355.383156	8.329984	-0.106665	4.303376
554.094553	6363.471206	8.334989	-0.106706	4.306057
554.188709	6371.440328	8.339994	-0.106728	4.308696
554.315428	6379.537217	8.344998	-0.106757	4.311376
553.981966	6387.554135	8.350003	-0.106700	4.314025
554.308411	6395.504082	8.355008	-0.106766	4.316655
554.145114	6403.496338	8.360013	-0.106741	4.319293
554.481818	6411.464449	8.365018	-0.106809	4.321926
554.793871	6419.424893	8.370022	-0.106872	4.324554
554.850624	6427.541246	8.375027	-0.106888	4.327231
554.945626	6435.523374	8.380032	-0.106911	4.329861
554.920085	6443.589063	8.385037	-0.106911	4.332517
555.582391	6451.539546	8.390042	-0.107040	4.335138
555.744646	6459.543509	8.395046	-0.107075	4.337771
555.947603	6467.610405	8.400051	-0.107118	4.340424
556.538072	6475.546271	8.405056	-0.107233	4.343035
556.528735	6483.623155	8.410061	-0.107237	4.345686
556.595465	6491.658565	8.415066	-0.107254	4.348323
556.637602	6499.714662	8.420070	-0.107267	4.350964
557.273722	6507.751451	8.425075	-0.107391	4.353602
557.129505	6515.801446	8.430080	-0.107369	4.356237
557.294299	6523.768617	8.435085	-0.107405	4.358846
557.399944	6531.808713	8.440090	-0.107430	4.361476
557.268643	6539.716271	8.445094	-0.107411	4.364060
557.015373	6547.905352	8.450099	-0.107369	4.366733
557.140309	6555.793198	8.455104	-0.107397	4.369309
557.386617	6563.899624	8.460109	-0.107448	4.371956
557.651667	6571.875654	8.465114	-0.107503	4.374558
558.034010	6579.828352	8.470118	-0.107579	4.377152
558.234540	6587.870037	8.475123	-0.107622	4.379772
558.122175	6595.906382	8.480128	-0.107606	4.382387
558.781270	6603.846278	8.485133	-0.107734	4.384974
558.870921	6611.949889	8.490138	-0.107756	4.387609
559.010038	6620.007503	8.495142	-0.107787	4.390228
559.170538	6628.034007	8.500147	-0.107822	4.392835
559.257378	6636.042649	8.505152	-0.107843	4.395435
559.274009	6644.140165	8.510157	-0.107852	4.398061
559.535239	6652.084930	8.515162	-0.107905	4.400637
559.800465	6660.055602	8.520166	-0.107960	4.403221
560.109388	6668.101682	8.525171	-0.108023	4.405827
559.978573	6676.110132	8.530176	-0.108003	4.408418
560.392270	6684.176640	8.535181	-0.108086	4.411028
560.831670	6692.145226	8.540186	-0.108173	4.413606
560.788808	6700.219604	8.545190	-0.108170	4.416213
560.593907	6708.244192	8.550195	-0.108139	4.418802
560.540907	6716.280763	8.555200	-0.108134	4.421395
561.175022	6724.216904	8.560205	-0.108257	4.423957
561.203916	6732.313982	8.565210	-0.108268	4.426566
561.244162	6740.296390	8.570215	-0.108281	4.429136
561.889851	6748.308904	8.575219	-0.108406	4.431718
561.839193	6756.305092	8.580224	-0.108402	4.434290
562.271595	6764.312129	8.585229	-0.108487	4.436866
562.112282	6772.303762	8.590234	-0.108463	4.439432
562.201326	6780.401313	8.595239	-0.108485	4.442033
562.001853	6788.399863	8.600243	-0.108453	4.444598
562.650540	6796.334186	8.605248	-0.108579	4.447146
562.714751	6804.385940	8.610253	-0.108596	4.449727
562.572079	6812.473594	8.615258	-0.108574	4.452317
562.930821	6820.402854	8.620263	-0.108646	4.454857
563.161537	6828.457623	8.625267	-0.108695	4.457435
562.982397	6836.485586	8.630272	-0.108666	4.460001
563.142818	6844.474497	8.635277	-0.108701	4.462555
563.454696	6852.439666	8.640282	-0.108765	4.465100
563.522812	6860.513433	8.645287	-0.108783	4.467678
563.630323	6868.544408	8.650291	-0.108808	4.470241
563.730592	6876.563482	8.655296	-0.108832	4.472798
564.154352	6884.569477	8.660301	-0.108916	4.475351
564.637483	6892.513800	8.665306	-0.109011	4.477883
564.730824	6900.536159	8.670311	-0.109033	4.480436
564.783091	6908.587185	8.675315	-0.109048	4.482998
564.725844	6916.609730	8.680320	-0.109043	4.485548
565.343371	6924.614410	8.685325	-0.109163	4.488094
565.277098	6932.685617	8.690330	-0.109156	4.490657
565.528453	6940.667404	8.695335	-0.109208	4.493191
565.459570	6948.750788	8.700339	-0.109200	4.495754
565.441328	6956.707214	8.705344	-0.109202	4.498277
565.993344	6964.731173	8.710349	-0.109310	4.500821
566.408738	6972.702120	8.715354	-0.109392	4.503346
566.461183	6980.702065	8.720359	-0.109407	4.505878
566.681102	6988.773022	8.725363	-0.109454	4.508432
566.631127	6996.828522	8.730368	-0.109449	4.510978
566.768377	7004.790918	8.735373	-0.109480	4.513494
566.909229	7012.817127	8.740378	-0.109512	4.516029
567.001489	7020.774129	8.745383	-0.109534	4.518540
566.662406	7028.914662	8.750387	-0.109476	4.521107
567.012131	7036.755552	8.755392	-0.109546	4.523579
567.418901	7044.855141	8.760397	-0.109627	4.526132
567.053206	7052.904349	8.765402	-0.109564	4.528666
567.467024	7060.861348	8.770407	-0.109646	4.531171
567.564638	7068.935618	8.775411	-0.109670	4.533711
567.593865	7076.922594	8.780416	-0.109680	4.536221
567.713546	7084.889482	8.785421	-0.109708	4.538724
567.676844	7092.985286	8.790426	-0.109706	4.541266
568.439611	7100.826206	8.795431	-0.109853	4.543729
568.301813	7108.988533	8.800435	-0.109833	4.546288
568.940771	7116.933042	8.805440	-0.109957	4.548780
569.328588	7125.013380	8.810445	-0.110035	4.551312
569.384707	7132.996739	8.815450	-0.110050	4.553812
569.309310	7141.085108	8.820455	-0.110041	4.556343
569.667216	7149.028620	8.825459	-0.110113	4.558828
569.933979	7157.099017	8.830464	-0.110168	4.561352
570.151330	7165.035324	8.835469	-0.110214	4.563831
569.686755	7173.161688	8.840474	-0.110132	4.566368
570.494317	7181.078744	8.845479	-0.110288	4.568840
570.109061	7189.222549	8.850483	-0.110221	4.571379
570.961228	7197.075373	8.855488	-0.110385	4.573829
571.008853	7205.210032	8.860493	-0.110399	4.576363
571.155557	7213.151224	8.865498	-0.110432	4.578836
570.773918	7221.294634	8.870503	-0.110366	4.581370
570.833230	7229.233847	8.875507	-0.110382	4.583839
570.738665	7237.289453	8.880512	-0.110370	4.586343
571.166552	7245.254102	8.885517	-0.110455	4.588819
571.718065	7253.272089	8.890522	-0.110562	4.591309
571.919941	7261.243436	8.895527	-0.110605	4.593783
571.969664	7269.377679	8.900531	-0.110620	4.596306
571.867636	7277.275086	8.905536	-0.110606	4.598755
571.927012	7285.390923	8.910541	-0.110622	4.601269
572.476916	7293.224688	8.915546	-0.110730	4.603696
572.056877	7301.336331	8.920551	-0.110657	4.606206
572.513646	7309.342482	8.925555	-0.110747	4.608683
572.796508	7317.349399	8.930560	-0.110805	4.611159
572.568801	7325.450485	8.935565	-0.110767	4.613662
573.213394	7333.401985	8.940570	-0.110893	4.616118
573.246193	7341.401208	8.945575	-0.110904	4.618588
573.403517	7349.421814	8.950579	-0.110938	4.621062
573.556304	7357.406281	8.955584	-0.110972	4.623524
573.651469	7365.506572	8.960589	-0.110995	4.626020
573.776638	7373.537259	8.965594	-0.111023	4.628494
574.109760	7381.480953	8.970599	-0.111091	4.630939
574.571039	7389.485817	8.975603	-0.111182	4.633402
574.477009	7397.523472	8.980608	-0.111169	4.635874
574.298289	7405.535892	8.985613	-0.111141	4.638337
575.104186	7413.524588	8.990618	-0.111297	4.640791
575.091305	7421.506032	8.995623	-0.111299	4.643241
575.222540	7429.630238	9.000627	-0.111329	4.645734
575.406062	7437.590917	9.005632	-0.111368	4.648175
575.554629	7445.688254	9.010637	-0.111401	4.650657
575.558435	7453.677636	9.015642	-0.111407	4.653105
575.419492	7461.673027	9.020647	-0.111386	4.655553
575.537060	7469.704706	9.025651	-0.111413	4.658011
575.735370	7477.691846	9.030656	-0.111456	4.660454
575.902649	7485.697491	9.035661	-0.111492	4.662902
576.273294	7493.669087	9.040666	-0.111566	4.665337
576.581924	7501.709255	9.045671	-0.111629	4.667792
576.813931	7509.799603	9.050675	-0.111677	4.670261
576.551512	7517.818072	9.055680	-0.111633	4.672708
576.740011	7525.839061	9.060685	-0.111674	4.675153
577.022819	7533.891303	9.065690	-0.111732	4.677607
576.904227	7541.865416	9.070695	-0.111715	4.680036
577.142934	7549.837837	9.075699	-0.111764	4.682462
577.272949	7557.756577	9.080704	-0.111794	4.684872
577.730514	7565.864660	9.085709	-0.111884	4.687337
577.522843	7573.900253	9.090714	-0.111851	4.689779
577.754210	7581.933785	9.095719	-0.111899	4.692220
577.974896	7589.890293	9.100723	-0.111945	4.694635
578.282694	7597.898767	9.105728	-0.112008	4.697065
578.144003	7605.896818	9.110733	-0.111987	4.699491
578.453547	7613.989985	9.115738	-0.112050	4.701944
578.522879	7621.910941	9.120743	-0.112068	4.704344
578.603209	7630.057745	9.125747	-0.112088	4.706811
578.148718	7638.072547	9.130752	-0.112009	4.709238
578.694623	7646.135732	9.135757	-0.112115	4.711676
579.010095	7654.092358	9.140762	-0.112179	4.714081
578.917379	7662.143478	9.145767	-0.112167	4.716514
579.712007	7670.013503	9.150771	-0.112320	4.718890
579.673829	7678.141610	9.155776	-0.112318	4.721344
579.499797	7686.132208	9.160781	-0.112291	4.723755
579.821925	7694.148102	9.165786	-0.112356	4.726172
580.414993	7702.074975	9.170791	-0.112472	4.728560
580.415119	7710.172505	9.175795	-0.112477	4.731000
580.766337	7718.185762	9.180800	-0.112548	4.733412
580.457590	7726.251807	9.185805	-0.112495	4.735840
580.566866	7734.272436	9.190810	-0.112521	4.738252
580.675662	7742.280580	9.195815	-0.112546	4.740660
581.091885	7750.284108	9.200819	-0.112629	4.743064
581.129747	7758.229209	9.205824	-0.112641	4.745450
581.171097	7766.330242	9.210829	-0.112654	4.747882
580.958640	7774.356060	9.215834	-0.112620	4.750290
581.309943	7782.329819	9.220839	-0.112690	4.752680
581.389085	7790.426984	9.225843	-0.112710	4.755107
581.606087	7798.387926	9.230848	-0.112756	4.757491
582.230104	7806.304931	9.235853	-0.112877	4.759860
582.329216	7814.355311	9.240858	-0.112901	4.762269
582.270501	7822.332986	9.245863	-0.112895	4.764655
582.582429	7830.463807	9.250867	-0.112958	4.767085
582.793035	7838.396103	9.255872	-0.113003	4.769455
582.779634	7846.541151	9.260877	-0.113006	4.771888
582.824180	7854.477605	9.265882	-0.113019	4.774256
583.014261	7862.525411	9.270887	-0.113060	4.776657
582.936641	7870.530233	9.275891	-0.113050	4.779044
583.532476	7878.460086	9.280896	-0.113166	4.781406
583.456730	7886.483462	9.285901	-0.113158	4.783796
583.881295	7894.513830	9.290906	-0.113242	4.786186
583.931961	7902.513287	9.295911	-0.113256	4.788567
584.332388	7910.613570	9.300915	-0.113336	4.790975
584.416598	7918.550165	9.305920	-0.113357	4.793334
584.242708	7926.605034	9.310925	-0.113330	4.795728
584.323130	7934.635702	9.315930	-0.113350	4.798113
584.791812	7942.576748	9.320935	-0.113442	4.800469
584.740479	7950.675806	9.325939	-0.113438	4.802872
584.510424	7958.639547	9.330944	-0.113400	4.805235
585.036909	7966.652517	9.335949	-0.113504	4.807608
585.639703	7974.674961	9.340954	-0.113621	4.809982
585.369196	7982.668962	9.345959	-0.113576	4.812350
585.353212	7990.159883	9.350963	-0.113578	4.814567
585.412787	7994.670620	9.355968	-0.113592	4.815902

585.723299	7997.217707	9.360973	-0.113651	4.816654
585.895948	7998.479531	9.365978	-0.113684	4.817026
586.012616	7998.908779	9.370983	-0.113706	4.817153
586.283428	7999.924119	9.375987	-0.113757	4.817452
586.483072	7999.895411	9.380992	-0.113794	4.817443
586.562452	7999.870195	9.385997	-0.113809	4.817435
586.579966	7999.901067	9.391002	-0.113812	4.817444
586.163344	7999.925488	9.396007	-0.113734	4.817453
586.628989	7999.931349	9.401011	-0.113821	4.817453
586.643878	7999.933678	9.406016	-0.113824	4.817453
587.104406	7999.919406	9.411021	-0.113910	4.817447
587.037086	7999.936349	9.416026	-0.113897	4.817452
586.929157	7999.938964	9.421031	-0.113877	4.817453
587.317567	7999.885615	9.426035	-0.113949	4.817436
587.212339	7999.879824	9.431040	-0.113929	4.817435
586.948969	7999.921302	9.436045	-0.113880	4.817448
587.183498	7999.940621	9.441050	-0.113924	4.817453
587.378076	7999.877000	9.446055	-0.113960	4.817433
587.041643	7999.984957	9.451059	-0.113898	4.817467
587.329350	7999.975506	9.456064	-0.113951	4.817463
587.272902	7999.910265	9.461069	-0.113941	4.817443
587.138803	8000.024397	9.466074	-0.113916	4.817478
587.471139	7999.943821	9.471079	-0.113977	4.817453
587.656931	7999.995145	9.476083	-0.114012	4.817467
587.535819	7999.946888	9.481088	-0.113989	4.817453
587.204746	8000.005305	9.486093	-0.113928	4.817472
587.493237	8000.026484	9.491098	-0.113981	4.817477
587.519712	7999.951917	9.496103	-0.113986	4.817455
587.917016	7999.932484	9.501107	-0.114060	4.817447
587.937882	7999.933847	9.506112	-0.114064	4.817448
588.109382	7999.906834	9.511117	-0.114096	4.817439
588.350309	7999.894577	9.516122	-0.114141	4.817434
588.229871	7999.878002	9.521127	-0.114118	4.817430
588.106793	7999.987021	9.526131	-0.114095	4.817463
588.262949	7999.942888	9.531136	-0.114124	4.817449
588.324208	7999.975468	9.536141	-0.114136	4.817458
588.286130	8000.036132	9.541146	-0.114129	4.817476
588.040235	7999.935342	9.546151	-0.114083	4.817448
588.082970	8000.005654	9.551155	-0.114091	4.817468
588.487327	7999.872306	9.556160	-0.114166	4.817427
588.661317	7999.852720	9.561165	-0.114198	4.817420
588.888989	7999.869829	9.566170	-0.114241	4.817424
588.637763	7999.885092	9.571175	-0.114194	4.817430
588.551287	7999.940812	9.576179	-0.114178	4.817447
588.771178	7999.845895	9.581184	-0.114218	4.817418
588.291912	7999.968620	9.586189	-0.114129	4.817456
588.338362	7999.995701	9.591194	-0.114138	4.817464
588.462512	7999.934200	9.596199	-0.114161	4.817445
588.551773	7999.930245	9.601203	-0.114177	4.817444
588.767236	7999.888050	9.606208	-0.114218	4.817430
588.713804	7999.918924	9.611213	-0.114208	4.817440
588.249541	8000.036593	9.616218	-0.114121	4.817477
588.683625	7999.927970	9.621223	-0.114202	4.817443
588.320654	8000.042923	9.626227	-0.114134	4.817478
588.657382	7999.995142	9.631232	-0.114197	4.817463
588.840787	7999.965139	9.636237	-0.114231	4.817453
588.979636	7999.970368	9.641242	-0.114257	4.817454
589.359683	7999.851440	9.646247	-0.114327	4.817417
589.084635	7999.921247	9.651251	-0.114276	4.817439
589.196496	7999.897570	9.656256	-0.114297	4.817431
589.540732	7999.860458	9.661261	-0.114361	4.817419
589.219469	7999.870455	9.666266	-0.114301	4.817423
589.066124	7999.839665	9.671271	-0.114273	4.817415
589.643708	7999.839809	9.676275	-0.114380	4.817412
589.564343	7999.810119	9.681280	-0.114365	4.817404
589.439831	7999.819877	9.686285	-0.114342	4.817407
589.604462	7999.839215	9.691290	-0.114373	4.817412
589.560946	7999.806891	9.696295	-0.114365	4.817403
589.629330	7999.839579	9.701299	-0.114377	4.817412
589.932838	7999.821921	9.706304	-0.114434	4.817406
589.954437	7999.823295	9.711309	-0.114438	4.817406
589.419344	7999.923017	9.716314	-0.114338	4.817438
589.376370	7999.825243	9.721319	-0.114330	4.817409
589.649855	7999.867317	9.726323	-0.114381	4.817420
589.472469	7999.848838	9.731328	-0.114348	4.817416
589.249230	7999.906747	9.736333	-0.114306	4.817434
589.641077	7999.874567	9.741338	-0.114379	4.817423
589.901706	7999.831988	9.746343	-0.114428	4.817409
589.373766	7999.864248	9.751347	-0.114329	4.817421
589.292811	7999.869375	9.756352	-0.114314	4.817423
589.768364	7999.828938	9.761357	-0.114403	4.817409
590.077085	7999.818748	9.766362	-0.114460	4.817404
589.808882	7999.804196	9.771367	-0.114410	4.817401
589.448988	7999.923418	9.776371	-0.114343	4.817438
589.505783	7999.884140	9.781376	-0.114354	4.817426
589.853752	7999.828080	9.786381	-0.114418	4.817408
589.554627	7999.935538	9.791386	-0.114363	4.817441
589.629517	7999.831071	9.796391	-0.114376	4.817410
589.774641	7999.884961	9.801395	-0.114403	4.817425
589.512296	7999.918005	9.806400	-0.114355	4.817436
589.591623	7999.863226	9.811405	-0.114369	4.817419
589.645256	7999.904141	9.816410	-0.114379	4.817431
589.534312	7999.869757	9.821415	-0.114359	4.817422
589.568366	7999.890320	9.826419	-0.114365	4.817428
589.678210	7999.844442	9.831424	-0.114385	4.817414
589.894433	7999.839210	9.836429	-0.114425	4.817411
589.775424	7999.878611	9.841434	-0.114403	4.817423
589.806747	7999.826285	9.846439	-0.114409	4.817408
590.120980	7999.873190	9.851443	-0.114468	4.817420
589.306859	7999.887464	9.856448	-0.114316	4.817428
589.740565	7999.856963	9.861453	-0.114397	4.817417
589.751253	7999.891959	9.866458	-0.114399	4.817427
589.442017	7999.878908	9.871463	-0.114341	4.817425
589.634157	7999.928218	9.876467	-0.114377	4.817438
589.988099	7999.857466	9.881472	-0.114443	4.817416
589.997030	7999.855484	9.886477	-0.114444	4.817415
590.172169	7999.851753	9.891482	-0.114477	4.817414
590.085024	7999.844118	9.896487	-0.114460	4.817412
590.182374	7999.864568	9.901491	-0.114479	4.817417
590.110581	7999.857161	9.906496	-0.114465	4.817415
590.468051	7999.856144	9.911501	-0.114532	4.817414
590.128251	7999.922876	9.916506	-0.114468	4.817435
589.360815	7999.952625	9.921511	-0.114325	4.817447
589.984888	7999.874281	9.926515	-0.114442	4.817421
589.758807	7999.905753	9.931520	-0.114399	4.817431
589.982919	7999.892193	9.936525	-0.114441	4.817426
590.074591	7999.873494	9.941530	-0.114458	4.817420
589.676225	7999.921406	9.946535	-0.114384	4.817436
589.850474	7999.932443	9.951539	-0.114416	4.817439
589.846842	7999.941888	9.956544	-0.114416	4.817442
589.830149	7999.940580	9.961549	-0.114412	4.817441
590.074895	7999.885096	9.966554	-0.114458	4.817424
590.146780	7999.875605	9.971559	-0.114471	4.817421
590.404613	7999.883663	9.976563	-0.114519	4.817422
590.364027	7999.867218	9.981568	-0.114512	4.817417
590.294292	7999.870400	9.986573	-0.114499	4.817418
589.940758	7999.939039	9.991578	-0.114433	4.817440
590.118710	7999.895230	9.996583	-0.114466	4.817427
590.083333	7999.962270	10.001587	-0.114459	4.817447
590.434880	7999.887260	10.006592	-0.114525	4.817423
590.635085	7999.877568	10.011597	-0.114562	4.817419
590.523549	7999.907578	10.016602	-0.114541	4.817428
590.169147	7999.909689	10.021607	-0.114475	4.817431
590.436203	7999.872485	10.026611	-0.114525	4.817418
590.710679	7999.840671	10.031616	-0.114576	4.817408
590.856031	7999.874506	10.036621	-0.114603	4.817417
590.226535	7999.969654	10.041626	-0.114486	4.817448
590.062419	7999.932367	10.046631	-0.114455	4.817438
590.411448	7999.902718	10.051635	-0.114520	4.817428
590.170579	7999.952974	10.056640	-0.114475	4.817443
590.357941	7999.885022	10.061645	-0.114510	4.817423
590.499777	7999.965260	10.066650	-0.114536	4.817446
590.586662	7999.862026	10.071655	-0.114552	4.817415
590.643331	7999.858643	10.076659	-0.114563	4.817414
590.665244	7999.934983	10.081664	-0.114567	4.817436
590.351824	7999.904974	10.086669	-0.114509	4.817428
590.433820	7999.955814	10.091674	-0.114524	4.817443
590.002504	7999.956780	10.096679	-0.114443	4.817445
590.090591	7999.959144	10.101683	-0.114460	4.817446
590.449253	7999.902188	10.106688	-0.114527	4.817427
590.250730	7999.889727	10.111693	-0.114490	4.817424
590.331090	8000.003890	10.116698	-0.114504	4.817458
590.417327	7999.905926	10.121703	-0.114520	4.817428
590.493297	7999.927114	10.126707	-0.114535	4.817434
590.550785	7999.899460	10.131712	-0.114545	4.817426
590.827420	7999.834948	10.136717	-0.114597	4.817406
590.715451	7999.898737	10.141722	-0.114576	4.817425
590.294959	7999.920980	10.146727	-0.114497	4.817433
590.678612	7999.864397	10.151731	-0.114569	4.817415
590.924493	7999.828990	10.156736	-0.114615	4.817404
590.710246	7999.862749	10.161741	-0.114575	4.817414
591.302207	7999.827217	10.166746	-0.114685	4.817401
590.643259	7999.849076	10.171751	-0.114562	4.817411
590.708006	7999.873264	10.176755	-0.114574	4.817418
590.615395	7999.900388	10.181760	-0.114557	4.817426
590.467828	7999.865458	10.186765	-0.114529	4.817416
590.516888	7999.940091	10.191770	-0.114538	4.817438
590.420434	7999.882694	10.196775	-0.114520	4.817422
590.447348	7999.907375	10.201779	-0.114525	4.817429
590.745601	7999.879082	10.206784	-0.114581	4.817419
590.438375	7999.875561	10.211789	-0.114524	4.817419
590.689826	7999.940538	10.216794	-0.114570	4.817438
590.420862	7999.918581	10.221799	-0.114520	4.817432
590.555602	7999.915305	10.226803	-0.114545	4.817431
590.491343	8000.015701	10.231808	-0.114533	4.817461
590.206451	7999.963945	10.236813	-0.114480	4.817447
590.051578	8000.085164	10.241818	-0.114451	4.817483
590.136418	8000.042080	10.246823	-0.114467	4.817470
590.436178	7999.987416	10.251827	-0.114523	4.817453
590.086733	8000.040278	10.256832	-0.114458	4.817470
590.406917	7999.958467	10.261837	-0.114517	4.817444
590.629062	7999.968106	10.266842	-0.114559	4.817446
590.396415	7999.869617	10.271847	-0.114515	4.817418
590.842648	7999.853029	10.276851	-0.114598	4.817411
591.071896	7999.869109	10.281856	-0.114641	4.817415
590.662317	7999.902072	10.286861	-0.114565	4.817426
590.323305	8000.013159	10.291866	-0.114502	4.817461
590.526305	7999.893705	10.296871	-0.114539	4.817424
590.838938	7999.903636	10.301875	-0.114597	4.817426
590.598965	7999.922231	10.306880	-0.114553	4.817433
590.773463	7999.892096	10.311885	-0.114585	4.817423
591.202703	7999.924880	10.316890	-0.114665	4.817431
590.407620	8000.009115	10.321895	-0.114517	4.817459
590.292037	8000.012670	10.326899	-0.114495	4.817461
590.566733	8000.023092	10.331904	-0.114547	4.817463
590.482842	7999.969049	10.336909	-0.114531	4.817447
590.468550	8000.030069	10.341914	-0.114528	4.817465
590.391233	7999.939171	10.346919	-0.114514	4.817438
590.702755	7999.892072	10.351923	-0.114572	4.817423
590.552517	7999.976408	10.356928	-0.114544	4.817449
590.709323	7999.911168	10.361933	-0.114573	4.817429
590.670137	7999.973929	10.366938	-0.114566	4.817448
590.775033	7999.934311	10.371943	-0.114585	4.817435
590.574046	7999.967213	10.376947	-0.114548	4.817446
590.853464	7999.960812	10.381952	-0.114600	4.817443
590.826394	7999.900224	10.386957	-0.114594	4.817425
591.105442	7999.909656	10.391962	-0.114646	4.817427
591.225052	7999.857587	10.396967	-0.114669	4.817411
591.397805	7999.877050	10.401971	-0.114701	4.817416
590.983274	7999.887766	10.406976	-0.114623	4.817421
591.066673	7999.837270	10.411981	-0.114639	4.817405
591.395092	7999.857995	10.416986	-0.114700	4.817410
591.456348	7999.831452	10.421991	-0.114711	4.817402
591.400964	7999.866522	10.426995	-0.114701	4.817413
591.088856	7999.895656	10.432000	-0.114643	4.817423
591.175123	7999.878989	10.437005	-0.114659	4.817417
591.395929	7999.897055	10.442010	-0.114700	4.817422
591.693711	7999.823357	10.447015	-0.114755	4.817399
591.582096	7999.831193	10.452019	-0.114735	4.817401
591.292829	7999.876505	10.457024	-0.114681	4.817416
591.045333	7999.873872	10.462029	-0.114635	4.817416
591.333125	7999.929889	10.467034	-0.114688	4.817432
591.055058	7999.934191	10.472039	-0.114636	4.817434
591.087246	7999.904048	10.477043	-0.114642	4.817425
590.947974	7999.909362	10.482048	-0.114616	4.817427
591.340992	7999.871923	10.487053	-0.114689	4.817414
591.285222	7999.912266	10.492058	-0.114679	4.817427
591.161505	7999.874522	10.497063	-0.114656	4.817416
591.019569	7999.907247	10.502067	-0.114629	4.817426
591.221542	7999.916586	10.507072	-0.114667	4.817428
591.256772	7999.855871	10.512077	-0.114673	4.817410
591.585131	7999.878707	10.517082	-0.114735	4.817415
591.562855	7999.825580	10.522087	-0.114730	4.817400
591.602516	7999.846228	10.527091	-0.114738	4.817406
591.294430	7999.849027	10.532096	-0.114680	4.817408
591.127939	7999.846544	10.537101	-0.114649	4.817408
591.814836	7999.857827	10.542106	-0.114777	4.817408
591.906354	7999.838071	10.547111	-0.114794	4.817402
591.673979	7999.871560	10.552115	-0.114751	4.817413
591.326070	7999.860040	10.557120	-0.114686	4.817411
591.408027	7999.862313	10.562125	-0.114701	4.817411
591.829470	7999.862252	10.567130	-0.114780	4.817409
591.722826	7999.841655	10.572135	-0.114760	4.817404
591.792081	7999.835293	10.577139	-0.114773	4.817402
592.040904	7999.797818	10.582144	-0.114819	4.817389
592.038607	7999.799893	10.587149	-0.114818	4.817390
592.054201	7999.825461	10.592154	-0.114821	4.817398
592.095882	7999.822911	10.597159	-0.114829	4.817397
591.933460	7999.855331	10.602163	-0.114799	4.817407
591.787878	7999.866885	10.607168	-0.114772	4.817411
591.731574	7999.850205	10.612173	-0.114761	4.817406
591.639976	7999.842502	10.617178	-0.114744	4.817404
591.514581	7999.850134	10.622183	-0.114721	4.817407
591.615412	7999.879084	10.627187	-0.114739	4.817415
591.784861	7999.839371	10.632192	-0.114771	4.817403
591.518888	7999.831183	10.637197	-0.114721	4.817402
591.636190	7999.855099	10.642202	-0.114743	4.817408
591.901003	7999.814696	10.647207	-0.114792	4.817395
591.605005	7999.896861	10.652211	-0.114737	4.817421
591.591239	7999.897708	10.657216	-0.114735	4.817421
591.299787	7999.878582	10.662221	-0.114680	4.817417
591.253056	7999.941232	10.667226	-0.114671	4.817435
591.405147	7999.875921	10.672231	-0.114700	4.817415
591.276690	7999.875061	10.677235	-0.114676	4.817416
591.256577	7999.907488	10.682240	-0.114672	4.817425
590.580625	7999.967102	10.687245	-0.114546	4.817446
591.134126	7999.932053	10.692250	-0.114649	4.817433
591.479971	7999.839010	10.697255	-0.114713	4.817404
591.554863	7999.853847	10.702259	-0.114727	4.817408
591.719588	7999.861577	10.707264	-0.114758	4.817410
591.783954	7999.829801	10.712269	-0.114770	4.817400
591.411110	7999.936162	10.717274	-0.114701	4.817433
591.785975	7999.845662	10.722279	-0.114770	4.817405
591.526586	7999.857633	10.727283	-0.114722	4.817409
591.280349	7999.884580	10.732288	-0.114676	4.817418
591.801103	7999.849045	10.737293	-0.114773	4.817406
591.723375	7999.875335	10.742298	-0.114758	4.817414
591.788932	7999.847801	10.747303	-0.114771	4.817405
591.269848	7999.924532	10.752307	-0.114674	4.817430
591.443109	7999.933444	10.757312	-0.114706	4.817432
591.025461	7999.951504	10.762317	-0.114628	4.817439
590.944021	7999.975627	10.767322	-0.114613	4.817447
591.412556	7999.904472	10.772327	-0.114700	4.817424
591.096627	7999.932493	10.777331	-0.114641	4.817433
591.050470	7999.950807	10.782336	-0.114633	4.817439
591.528494	7999.848118	10.787341	-0.114722	4.817407
591.374768	7999.911286	10.792346	-0.114693	4.817426
591.398945	7999.909531	10.797351	-0.114698	4.817425
591.435496	7999.935412	10.802355	-0.114704	4.817433
591.490246	7999.941503	10.807360	-0.114714	4.817434
591.202919	7999.926662	10.812365	-0.114661	4.817431
591.469748	7999.939079	10.817370	-0.114711	4.817434
591.647753	7999.910053	10.822375	-0.114744	4.817424
591.483920	7999.926614	10.827379	-0.114713	4.817430
591.313015	7999.912451	10.832384	-0.114681	4.817427
591.455527	7999.874449	10.837389	-0.114708	4.817415
591.630418	7999.941456	10.842394	-0.114740	4.817434
591.209463	7999.976359	10.847399	-0.114662	4.817446
591.373623	7999.920731	10.852403	-0.114692	4.817429
591.177241	8000.000156	10.857408	-0.114656	4.817453
591.382469	7999.917688	10.862413	-0.114694	4.817428
591.474069	7999.979231	10.867418	-0.114711	4.817446
591.684279	7999.895782	10.872423	-0.114750	4.817420
591.754324	7999.903157	10.877427	-0.114763	4.817422
591.888517	7999.891427	10.882432	-0.114788	4.817418
591.896718	7999.873596	10.887437	-0.114789	4.817413
592.279299	7999.868735	10.892442	-0.114861	4.817409
592.294625	7999.851010	10.897447	-0.114863	4.817404
592.282520	7999.856106	10.902451	-0.114861	4.817406
592.265109	7999.880127	10.907456	-0.114858	4.817413
592.319962	7999.841875	10.912461	-0.114868	4.817401
592.249540	7999.876721	10.917466	-0.114855	4.817412
592.066571	7999.866601	10.922471	-0.114821	4.817410
591.870378	7999.906964	10.927475	-0.114784	4.817423
591.799506	7999.920686	10.932480	-0.114771	4.817427
592.139633	7999.829669	10.937485	-0.114834	4.817399
591.696137	7999.957149	10.942490	-0.114752	4.817438
591.680005	7999.945291	10.947495	-0.114749	4.817435
592.144463	7999.856127	10.952499	-0.114835	4.817406
591.989996	7999.861213	10.957504	-0.114806	4.817409
592.244471	7999.840717	10.962509	-0.114854	4.817401
592.014877	7999.887973	10.967514	-0.114811	4.817416
591.975268	7999.876821	10.972519	-0.114803	4.817413
591.823265	7999.896726	10.977523	-0.114775	4.817420
591.688115	7999.966505	10.982528	-0.114750	4.817441
591.195119	7999.940153	10.987533	-0.114658	4.817435
591.340018	7999.983485	10.992538	-0.114685	4.817448
591.689782	7999.878886	10.997543	-0.114750	4.817415
591.803561	7999.891136	11.002547	-0.114771	4.817418
591.919417	7999.908696	11.007552	-0.114793	4.817423
591.982701	7999.856844	11.012557	-0.114804	4.817407
591.892038	7999.926231	11.017562	-0.114788	4.817428
591.638251	7999.924558	11.022567	-0.114740	4.817429
591.766534	7999.894791	11.027571	-0.114764	4.817419
592.053071	7999.920173	11.032576	-0.114817	4.817426
591.946236	7999.879512	11.037581	-0.114797	4.817414
592.248671	7999.898797	11.042586	-0.114854	4.817418
592.077629	7999.894133	11.047591	-0.114822	4.817418
592.157353	7999.845693	11.052595	-0.114837	4.817403
592.402817	7999.854626	11.057600	-0.114882	4.817405
591.989555	7999.876973	11.062605	-0.114805	4.817413
592.186477	7999.907356	11.067610	-0.114842	4.817421
591.823759	7999.905116	11.072615	-0.114774	4.817422
592.031625	7999.892372	11.077619	-0.114813	4.817418
591.583950	7999.956439	11.082624	-0.114730	4.817438
591.568576	7999.922421	11.087629	-0.114727	4.817428
591.607877	7999.926170	11.092634	-0.114734	4.817429
591.603820	7999.967284	11.097639	-0.114733	4.817442
591.744977	7999.941932	11.102643	-0.114759	4.817433
591.743086	7999.963017	11.107648	-0.114759	4.817440
591.786559	7999.942544	11.112653	-0.114767	4.817433
591.893949	7999.953643	11.117658	-0.114787	4.817436
592.088326	7999.902689	11.122663	-0.114823	4.817420
591.869802	7999.945886	11.127667	-0.114782	4.817434
592.113658	7999.980136	11.132672	-0.114828	4.817443
591.920936	7999.897017	11.137677	-0.114792	4.817419
591.890837	7999.968362	11.142682	-0.114786	4.817441
592.007050	8000.018659	11.147687	-0.114808	4.817455
592.109462	7999.910374	11.152691	-0.114827	4.817423
591.899500	7999.932583	11.157696	-0.114788	4.817430
591.711392	7999.923442	11.162701	-0.114753	4.817428
592.012757	7999.949045	11.167706	-0.114809	4.817434
591.825604	7999.951532	11.172711	-0.114774	4.817436
592.104327	7999.889164	11.177715	-0.114826	4.817416
592.071142	7999.914006	11.182720	-0.114819	4.817424
591.965745	7999.896595	11.187725	-0.114800	4.817419
592.166715	7999.908033	11.192730	-0.114837	4.817422
592.653031	7999.861428	11.197735	-0.114928	4.817406
592.130925	7999.903269	11.202739	-0.114830	4.817420
592.366542	7999.896218	11.207744	-0.114874	4.817417
592.364921	7999.855013	11.212749	-0.114874	4.817405
592.657364	7999.884708	11.217754	-0.114928	4.817413
591.910076	7999.981265	11.222759	-0.114789	4.817444
592.023314	7999.938603	11.227763	-0.114810	4.817431
592.212341	7999.934026	11.232768	-0.114845	4.817429
591.699177	7999.981280	11.237773	-0.114750	4.817445
592.220044	7999.958418	11.242778	-0.114847	4.817436
592.020809	8000.014573	11.247783	-0.114810	4.817454
591.498323	8000.000450	11.252787	-0.114712	4.817452
591.605176	8000.045328	11.257792	-0.114732	4.817465
591.980968	7999.929502	11.262797	-0.114802	4.817429
592.213722	7999.931911	11.267802	-0.114845	4.817428
592.514691	7999.890991	11.272807	-0.114901	4.817415
592.486130	7999.882116	11.277811	-0.114896	4.817413
592.548952	7999.887272	11.282816	-0.114908	4.817414
592.729493	7999.837166	11.287821	-0.114941	4.817398
592.305908	7999.904760	11.292826	-0.114862	4.817420
592.640231	7999.900236	11.297831	-0.114924	4.817417
592.697277	7999.864128	11.302835	-0.114935	4.817406
592.700853	7999.865234	11.307840	-0.114936	4.817407
592.554106	7999.850374	11.312845	-0.114908	4.817403
592.585035	7999.850831	11.317850	-0.114914	4.817403
592.436612	7999.865510	11.322855	-0.114886	4.817408
592.366631	7999.879245	11.327859	-0.114873	4.817412
592.263792	7999.909385	11.332864	-0.114854	4.817422
592.334281	7999.865031	11.337869	-0.114867	4.817408
592.050538	7999.918871	11.342874	-0.114814	4.817425
592.097140	7999.917450	11.347879	-0.114823	4.817425
591.848822	7999.940143	11.352883	-0.114777	4.817433
592.109655	7999.944026	11.357888	-0.114825	4.817433
591.681154	7999.949252	11.362893	-0.114745	4.817436
592.214924	7999.907577	11.367898	-0.114845	4.817421
592.219185	7999.937201	11.372903	-0.114845	4.817430
592.540640	7999.881805	11.377907	-0.114905	4.817412
592.206617	7999.929616	11.382912	-0.114843	4.817428
592.112389	7999.939823	11.387917	-0.114825	4.817431
592.427437	7999.903336	11.392922	-0.114884	4.817419
592.403443	7999.907199	11.397927	-0.114880	4.817420
592.526644	7999.892138	11.402931	-0.114902	4.817415
592.322779	7999.938721	11.407936	-0.114864	4.817430
592.011981	7999.953092	11.412941	-0.114807	4.817436
592.338230	7999.919939	11.417946	-0.114867	4.817424
592.330791	7999.909267	11.422951	-0.114866	4.817421
591.703684	7999.935818	11.427955	-0.114749	4.817432
592.096828	7999.967012	11.432960	-0.114822	4.817439
592.451905	7999.841376	11.437965	-0.114888	4.817401
592.827332	7999.844855	11.442970	-0.114958	4.817400
591.998175	7999.948639	11.447975	-0.114804	4.817434
592.088634	7999.946816	11.452979	-0.114820	4.817433
592.488273	7999.933763	11.457984	-0.114895	4.817428
592.293959	7999.886518	11.462989	-0.114859	4.817415
592.436720	7999.911871	11.467994	-0.114885	4.817422
592.274544	7999.918953	11.472999	-0.114855	4.817424
592.662187	7999.875102	11.478003	-0.114927	4.817410
592.916107	7999.848263	11.483008	-0.114974	4.817401
592.756646	7999.798370	11.488013	-0.114944	4.817387
592.458084	7999.879441	11.493018	-0.114889	4.817412
592.830663	7999.888158	11.498023	-0.114958	4.817413
592.528594	7999.863591	11.503027	-0.114902	4.817407
592.569408	7999.884257	11.508032	-0.114909	4.817413
592.525887	7999.838204	11.513037	-0.114901	4.817399
592.648253	7999.897040	11.518042	-0.114924	4.817416
592.690412	7999.877604	11.523047	-0.114932	4.817410
592.400556	7999.881728	11.528051	-0.114878	4.817413
592.525409	7999.888864	11.533056	-0.114901	4.817414
592.626844	7999.865032	11.538061	-0.114920	4.817407
592.665764	7999.902563	11.543066	-0.114927	4.817418
592.739009	7999.894149	11.548071	-0.114941	4.817415
592.695235	7999.890326	11.553075	-0.114933	4.817414
592.871292	7999.908784	11.558080	-0.114965	4.817419
592.650148	7999.862195	11.563085	-0.114924	4.817406
592.442200	7999.892880	11.568090	-0.114885	4.817416
592.548441	7999.902906	11.573095	-0.114905	4.817418
592.299979	7999.877028	11.578099	-0.114859	4.817412
592.072618	7999.989779	11.583104	-0.114816	4.817446
592.306159	7999.932017	11.588109	-0.114860	4.817428
592.294615	7999.926562	11.593114	-0.114858	4.817427
592.709563	7999.866224	11.598119	-0.114935	4.817407
592.350197	7999.924216	11.603123	-0.114868	4.817426
592.624946	7999.949424	11.608128	-0.114919	4.817432
592.350204	7999.916819	11.613133	-0.114868	4.817423
592.346490	7999.934709	11.618138	-0.114867	4.817429
592.620657	7999.916619	11.623143	-0.114918	4.817422
592.174850	7999.911028	11.628147	-0.114835	4.817423
592.441798	7999.919226	11.633152	-0.114885	4.817424
592.136191	7999.947400	11.638157	-0.114828	4.817433
591.717693	7999.953831	11.643162	-0.114750	4.817437
592.528735	7999.900450	11.648167	-0.114901	4.817418
592.624137	7999.878640	11.653171	-0.114918	4.817411
592.928807	7999.903239	11.658176	-0.114975	4.817417
592.667668	7999.861333	11.663181	-0.114926	4.817406
592.840550	7999.858626	11.668186	-0.114959	4.817404
592.951713	7999.855001	11.673191	-0.114979	4.817403
592.572754	7999.867299	11.678195	-0.114909	4.817408
592.757672	7999.868996	11.683200	-0.114943	4.817408
592.748758	7999.845631	11.688205	-0.114941	4.817401
592.883099	7999.866635	11.693210	-0.114966	4.817406
592.899067	7999.890098	11.698215	-0.114969	4.817413
592.661697	7999.868608	11.703219	-0.114925	4.817408
592.707800	7999.934754	11.708224	-0.114934	4.817427
592.455117	7999.932041	11.713229	-0.114887	4.817428
592.644211	7999.908459	11.718234	-0.114922	4.817420
592.610192	7999.872050	11.723239	-0.114915	4.817409
592.747843	7999.845590	11.728243	-0.114941	4.817401
592.666629	7999.895057	11.733248	-0.114926	4.817416
593.133562	7999.847108	11.738253	-0.115013	4.817399
593.202982	7999.853419	11.743258	-0.115025	4.817401
593.473998	7999.837394	11.748263	-0.115076	4.817395
593.408293	7999.812127	11.753267	-0.115064	4.817388
593.367460	7999.866419	11.758272	-0.115056	4.817404
593.146471	7999.865234	11.763277	-0.115015	4.817405
592.513702	7999.907536	11.768282	-0.114897	4.817420
592.876396	7999.896045	11.773287	-0.114964	4.817415
592.525182	7999.885528	11.778291	-0.114899	4.817414
592.664400	7999.920331	11.783296	-0.114925	4.817423
592.662024	7999.900231	11.788301	-0.114924	4.817417
593.206690	7999.889340	11.793306	-0.115026	4.817412
593.144136	7999.862008	11.798311	-0.115014	4.817404
593.265738	7999.824750	11.803315	-0.115037	4.817392
592.983684	7999.890229	11.808320	-0.114984	4.817413
592.995749	7999.846060	11.813325	-0.114986	4.817400
592.624038	7999.928152	11.818330	-0.114917	4.817426
592.902841	7999.887958	11.823335	-0.114969	4.817413
592.744188	7999.846524	11.828339	-0.114939	4.817401
592.686872	7999.879454	11.833344	-0.114929	4.817411
592.525459	7999.878101	11.838349	-0.114899	4.817411
592.842654	7999.887048	11.843354	-0.114958	4.817413
592.831477	7999.881599	11.848359	-0.114955	4.817411
592.450308	7999.941377	11.853363	-0.114884	4.817430
592.567798	8000.001197	11.858368	-0.114906	4.817448
591.928210	8000.030728	11.863373	-0.114787	4.817459
592.437596	7999.949625	11.868378	-0.114882	4.817433
592.473602	7999.996615	11.873383	-0.114889	4.817447
592.462463	7999.935207	11.878387	-0.114886	4.817428
592.319053	8000.044986	11.883392	-0.114860	4.817462
592.361251	7999.984372	11.888397	-0.114868	4.817443
592.759583	7999.865715	11.893402	-0.114942	4.817407
592.712073	7999.911461	11.898407	-0.114933	4.817420
592.221965	7999.943220	11.903411	-0.114842	4.817432
592.619560	7999.915355	11.908416	-0.114915	4.817422
592.764090	7999.914338	11.913421	-0.114942	4.817421
592.682051	7999.930005	11.918426	-0.114927	4.817426
593.017732	7999.911776	11.923431	-0.114989	4.817419
592.821165	7999.954245	11.928435	-0.114953	4.817433
592.998594	7999.939993	11.933440	-0.114986	4.817428
592.822872	7999.909918	11.938445	-0.114953	4.817419
593.030775	7999.946801	11.943450	-0.114992	4.817429
592.981115	7999.962951	11.948455	-0.114982	4.817434
592.674257	7999.959429	11.953459	-0.114925	4.817435
592.703821	7999.990487	11.958464	-0.114931	4.817444
592.644205	7999.976924	11.963469	-0.114920	4.817440
592.232221	8000.023573	11.968474	-0.114843	4.817456
592.890336	7999.979530	11.973479	-0.114965	4.817440
592.300585	7999.977072	11.978483	-0.114856	4.817442
592.541654	7999.969047	11.983488	-0.114900	4.817438
592.648672	7999.936852	11.988493	-0.114920	4.817428
592.854011	7999.897675	11.993498	-0.114958	4.817416
592.420291	7999.941888	11.998503	-0.114878	4.817431
592.837306	7999.934374	12.003507	-0.114955	4.817427
593.076892	7999.900986	12.008512	-0.115000	4.817416
592.964513	7999.917258	12.013517	-0.114979	4.817421
592.754738	7999.931021	12.018522	-0.114940	4.817426
593.348402	7999.902912	12.023527	-0.115050	4.817415
593.179759	7999.901450	12.028531	-0.115019	4.817415
593.182358	7999.912044	12.033536	-0.115019	4.817418
592.996680	7999.927223	12.038541	-0.114985	4.817424
593.343387	7999.917606	12.043546	-0.115049	4.817419
593.240246	7999.974137	12.048551	-0.115030	4.817437
592.816422	7999.975207	12.053555	-0.114951	4.817439
593.010172	7999.968589	12.058560	-0.114987	4.817436
593.044008	7999.932135	12.063565	-0.114993	4.817425
593.068258	7999.894482	12.068570	-0.114998	4.817414
593.140407	7999.914560	12.073575	-0.115011	4.817419
592.802420	7999.927468	12.078579	-0.114948	4.817425
593.023853	7999.915983	12.083584	-0.114989	4.817420
592.932861	7999.914624	12.088589	-0.114972	4.817420
593.158106	7999.876799	12.093594	-0.115014	4.817408
593.291161	7999.935796	12.098599	-0.115039	4.817425
592.960798	7999.896024	12.103603	-0.114977	4.817415
592.843228	7999.973458	12.108608	-0.114955	4.817438
593.412336	7999.895357	12.113613	-0.115061	4.817413
592.765739	7999.951179	12.118618	-0.114941	4.817432
592.678253	8000.011111	12.123623	-0.114925	4.817450
592.863239	7999.918838	12.128627	-0.114959	4.817422
593.288722	7999.887166	12.133632	-0.115038	4.817411
592.704250	7999.948137	12.138637	-0.114929	4.817431
592.976567	7999.904679	12.143642	-0.114980	4.817417
593.328269	7999.889857	12.148647	-0.115045	4.817411
592.930257	7999.881809	12.153651	-0.114971	4.817411
592.871917	7999.952735	12.158656	-0.114960	4.817432
593.233363	7999.893712	12.163661	-0.115028	4.817413
592.785612	7999.949330	12.168666	-0.114944	4.817431
593.070323	7999.972576	12.173671	-0.114997	4.817437
592.675560	7999.979358	12.178675	-0.114924	4.817441
592.650262	7999.981090	12.183680	-0.114919	4.817441
592.562239	7999.999836	12.188685	-0.114903	4.817447
592.728493	7999.960076	12.193690	-0.114933	4.817435
593.051420	7999.962774	12.198695	-0.114993	4.817434
593.002221	7999.907133	12.203699	-0.114984	4.817418
593.378206	7999.915902	12.208704	-0.115054	4.817419
592.817389	7999.955052	12.213709	-0.114950	4.817433
592.692494	7999.954243	12.218714	-0.114926	4.817433
593.016683	7999.955905	12.223719	-0.114987	4.817432
592.873024	7999.956927	12.228723	-0.114960	4.817433
592.915203	7999.946994	12.233728	-0.114968	4.817430
592.699695	7999.996571	12.238733	-0.114928	4.817446
592.807269	8000.000283	12.243738	-0.114948	4.817446
593.255956	7999.971069	12.248743	-0.115031	4.817436
593.138910	7999.898578	12.253747	-0.115009	4.817415
593.053870	7999.933206	12.258752	-0.114993	4.817425
592.917263	7999.955452	12.263757	-0.114968	4.817433
593.194350	7999.881445	12.268762	-0.115019	4.817409
593.353197	7999.921820	12.273767	-0.115049	4.817421
592.948977	7999.935853	12.278771	-0.114974	4.817427
593.210661	7999.966147	12.283776	-0.115022	4.817434
593.136939	7999.940760	12.288781	-0.115009	4.817427
593.241912	7999.939154	12.293786	-0.115028	4.817426
593.375198	7999.977037	12.298791	-0.115053	4.817437
593.477020	7999.902529	12.303795	-0.115072	4.817414
593.256416	7999.956254	12.308800	-0.115031	4.817431
593.532416	7999.938192	12.313805	-0.115082	4.817425
593.544081	7999.888736	12.318810	-0.115084	4.817410
593.541822	7999.895034	12.323815	-0.115084	4.817412
593.502033	7999.860650	12.328819	-0.115076	4.817402
593.239978	7999.930651	12.333824	-0.115027	4.817424
593.262884	7999.933101	12.338829	-0.115032	4.817424
592.859350	7999.990434	12.343834	-0.114957	4.817443
593.555429	7999.953293	12.348839	-0.115086	4.817429
593.173804	7999.948656	12.353843	-0.115015	4.817429
593.388213	7999.952905	12.358848	-0.115055	4.817430
593.297222	8000.056077	12.363853	-0.115038	4.817461
593.399571	7999.965738	12.368858	-0.115057	4.817433
593.044814	8000.054418	12.373863	-0.114991	4.817461
592.802476	7999.985339	12.378867	-0.114946	4.817442
593.037061	8000.003614	12.383872	-0.114989	4.817446
592.965234	8000.005708	12.388877	-0.114976	4.817447
593.180480	7999.905439	12.393882	-0.115016	4.817417
593.751901	7999.915010	12.398887	-0.115122	4.817417
593.513308	7999.898779	12.403891	-0.115078	4.817413
593.655873	7999.890342	12.408896	-0.115104	4.817410
593.241279	7999.919002	12.413901	-0.115027	4.817420
593.352883	7999.909048	12.418906	-0.115048	4.817417
593.422720	7999.945985	12.423911	-0.115061	4.817428
593.290053	7999.965121	12.428915	-0.115036	4.817434
593.269965	7999.960595	12.433920	-0.115032	4.817433
593.251531	7999.947646	12.438925	-0.115029	4.817429
592.921278	7999.921603	12.443930	-0.114967	4.817423
593.384936	7999.941181	12.448935	-0.115053	4.817426
593.190818	7999.927725	12.453939	-0.115017	4.817423
593.029677	7999.968610	12.458944	-0.114987	4.817436
592.997495	8000.006138	12.463949	-0.114981	4.817447
592.601987	8000.030859	12.468954	-0.114908	4.817456
593.063393	7999.975438	12.473959	-0.114993	4.817438
592.960363	7999.910547	12.478963	-0.114974	4.817419
593.483316	7999.920451	12.483968	-0.115071	4.817420
592.984358	7999.980585	12.488973	-0.114979	4.817440
593.255240	7999.898039	12.493978	-0.115029	4.817414
593.453282	7999.877759	12.498983	-0.115066	4.817407
593.540134	7999.873771	12.503987	-0.115082	4.817406
593.013255	7999.961997	12.508992	-0.114984	4.817434
593.002365	8000.024127	12.513997	-0.114982	4.817453
592.808265	7999.990610	12.519002	-0.114946	4.817443
593.176099	7999.932738	12.524007	-0.115014	4.817425
593.181841	7999.913815	12.529011	-0.115015	4.817419
593.155083	7999.973597	12.534016	-0.115010	4.817437
593.419941	7999.920525	12.539021	-0.115059	4.817420
593.154717	7999.922903	12.544026	-0.115010	4.817422
593.614250	7999.923415	12.549031	-0.115095	4.817420
593.370197	7999.925053	12.554035	-0.115050	4.817422
593.219024	7999.917516	12.559040	-0.115022	4.817420
593.405101	7999.902337	12.564045	-0.115056	4.817415
593.561891	7999.886722	12.569050	-0.115085	4.817409
593.561272	7999.903603	12.574055	-0.115085	4.817414
593.736402	7999.857640	12.579059	-0.115118	4.817400
593.510329	7999.886999	12.584064	-0.115076	4.817410
593.575636	7999.900639	12.589069	-0.115088	4.817414
593.632548	7999.887758	12.594074	-0.115098	4.817409
593.740438	7999.921040	12.599079	-0.115118	4.817419
593.599035	7999.891475	12.604083	-0.115092	4.817411
593.465939	7999.928555	12.609088	-0.115067	4.817422
593.838070	7999.900312	12.614093	-0.115136	4.817412
593.573993	7999.919600	12.619098	-0.115087	4.817419
593.723197	7999.915486	12.624103	-0.115115	4.817417
593.569830	7999.905805	12.629107	-0.115086	4.817415
593.612009	7999.925436	12.634112	-0.115094	4.817421
593.742015	7999.912589	12.639117	-0.115118	4.817416
593.412687	7999.921402	12.644122	-0.115057	4.817420
593.684620	7999.912782	12.649127	-0.115108	4.817417
593.442472	7999.909169	12.654131	-0.115062	4.817417
593.214330	7999.960669	12.659136	-0.115020	4.817433
593.250514	7999.971764	12.664141	-0.115027	4.817436
593.198876	7999.939315	12.669146	-0.115017	4.817427
593.543898	7999.902221	12.674151	-0.115081	4.817414
593.083747	7999.997776	12.679155	-0.114995	4.817444
593.511781	7999.926020	12.684160	-0.115075	4.817421
593.733757	7999.938829	12.689165	-0.115116	4.817424
593.528906	7999.952665	12.694170	-0.115078	4.817429
593.440965	7999.962965	12.699175	-0.115062	4.817433
593.401016	7999.959199	12.704179	-0.115054	4.817432
593.452659	7999.939904	12.709184	-0.115064	4.817426
593.093277	8000.047521	12.714189	-0.114997	4.817459
593.062226	7999.941468	12.719194	-0.114991	4.817428
593.473433	7999.991941	12.724199	-0.115068	4.817441
593.384396	7999.940984	12.729203	-0.115051	4.817426
593.656044	7999.923914	12.734208	-0.115102	4.817420
593.976781	7999.893849	12.739213	-0.115161	4.817410
593.942319	7999.894387	12.744218	-0.115155	4.817410
593.887169	7999.922070	12.749223	-0.115144	4.817418
593.797539	7999.905948	12.754227	-0.115128	4.817414
594.189401	7999.884335	12.759232	-0.115201	4.817406
594.267734	7999.859103	12.764237	-0.115215	4.817398
594.375394	7999.853314	12.769242	-0.115235	4.817396
594.583928	7999.874371	12.774247	-0.115274	4.817401
594.198784	7999.842226	12.779251	-0.115202	4.817394
594.173807	7999.887254	12.784256	-0.115197	4.817407
594.362190	7999.872109	12.789261	-0.115233	4.817402
594.117080	7999.906463	12.794266	-0.115187	4.817413
594.224829	7999.890116	12.799271	-0.115207	4.817408
594.221031	7999.872106	12.804275	-0.115206	4.817402
594.218151	7999.876283	12.809280	-0.115206	4.817404
594.030491	7999.918884	12.814285	-0.115171	4.817417
594.014139	7999.864787	12.819290	-0.115167	4.817401
594.255847	7999.913791	12.824295	-0.115212	4.817414
594.201043	7999.872847	12.829299	-0.115202	4.817403
594.155050	7999.874269	12.834304	-0.115194	4.817403
593.926645	7999.896201	12.839309	-0.115151	4.817411
594.081413	7999.844656	12.844314	-0.115180	4.817395
593.809208	7999.895499	12.849319	-0.115129	4.817411
594.164853	7999.846949	12.854323	-0.115195	4.817395
594.085183	7999.859484	12.859328	-0.115180	4.817399
594.255147	7999.867295	12.864333	-0.115212	4.817401
594.398802	7999.876825	12.869338	-0.115239	4.817403
594.306500	7999.875445	12.874343	-0.115221	4.817403
594.239354	7999.857546	12.879347	-0.115209	4.817398
594.058781	7999.881247	12.884352	-0.115175	4.817406
594.028795	7999.875517	12.889357	-0.115170	4.817404
593.930351	7999.862431	12.894362	-0.115151	4.817401
593.993217	7999.915104	12.899367	-0.115163	4.817416
594.134201	7999.864408	12.904371	-0.115189	4.817400
594.074002	7999.867731	12.909376	-0.115178	4.817402
594.063420	7999.886576	12.914381	-0.115176	4.817407
593.760293	7999.879941	12.919386	-0.115119	4.817407
594.026108	7999.897627	12.924391	-0.115169	4.817411
594.345868	7999.847486	12.929395	-0.115228	4.817394
594.187893	7999.896865	12.934400	-0.115199	4.817410
594.224513	7999.873123	12.939405	-0.115206	4.817403
594.163112	7999.860589	12.944410	-0.115194	4.817399
594.275391	7999.882322	12.949415	-0.115215	4.817405
594.330862	7999.862028	12.954419	-0.115225	4.817399
594.275031	7999.874919	12.959424	-0.115215	4.817403
594.314177	7999.862828	12.964429	-0.115222	4.817399
594.263779	7999.850459	12.969434	-0.115213	4.817396
594.545920	7999.889507	12.974439	-0.115265	4.817406
594.435882	7999.865689	12.979443	-0.115245	4.817399
594.223423	7999.882579	12.984448	-0.115205	4.817405
594.401007	7999.884168	12.989453	-0.115238	4.817405
594.210612	7999.869711	12.994458	-0.115203	4.817402
594.194029	7999.911695	12.999463	-0.115199	4.817414
593.854512	7999.942529	13.004467	-0.115136	4.817425
594.156933	7999.905856	13.009472	-0.115192	4.817413
594.343374	7999.891739	13.014477	-0.115227	4.817408
594.129896	7999.870602	13.019482	-0.115187	4.817402
594.076569	7999.901480	13.024487	-0.115177	4.817412
593.946694	7999.901652	13.029491	-0.115153	4.817412
594.345596	7999.904429	13.034496	-0.115227	4.817411
594.233942	7999.893258	13.039501	-0.115207	4.817409
593.879301	7999.903804	13.044506	-0.115140	4.817413
593.877638	7999.904832	13.049511	-0.115140	4.817414
594.198311	7999.877934	13.054515	-0.115200	4.817404
594.134052	7999.888587	13.059520	-0.115188	4.817408
594.147849	7999.918354	13.064525	-0.115190	4.817416
593.869780	7999.878304	13.069530	-0.115138	4.817406
594.302848	7999.910100	13.074535	-0.115219	4.817413
594.143568	7999.883436	13.079539	-0.115189	4.817406
593.598208	7999.952380	13.084544	-0.115088	4.817429
593.807732	7999.930160	13.089549	-0.115127	4.817421
594.164375	7999.851004	13.094554	-0.115193	4.817396
594.213783	7999.901364	13.099559	-0.115202	4.817411
594.204626	7999.887497	13.104563	-0.115201	4.817407
594.093822	7999.887953	13.109568	-0.115180	4.817408
594.292112	7999.901466	13.114573	-0.115217	4.817411
593.999916	7999.885490	13.119578	-0.115162	4.817407
594.193944	7999.904219	13.124583	-0.115198	4.817412
594.132347	7999.843111	13.129587	-0.115187	4.817394
594.061651	7999.866339	13.134592	-0.115174	4.817401
594.060722	7999.882160	13.139597	-0.115173	4.817406
593.658598	7999.911005	13.144602	-0.115099	4.817416
593.812316	7999.919629	13.149607	-0.115127	4.817418
594.017029	7999.849822	13.154611	-0.115165	4.817397
593.906372	7999.883013	13.159616	-0.115145	4.817407
594.007445	7999.887684	13.164621	-0.115163	4.817408
594.310829	7999.860528	13.169626	-0.115220	4.817399
594.102246	7999.922879	13.174631	-0.115181	4.817418
594.237193	7999.875262	13.179635	-0.115206	4.817403
594.260421	7999.890387	13.184640	-0.115210	4.817408
594.200760	7999.874712	13.189645	-0.115199	4.817403
594.252727	7999.837471	13.194650	-0.115209	4.817392
594.311199	7999.887967	13.199655	-0.115220	4.817407
594.254176	7999.867051	13.204659	-0.115209	4.817401
593.837348	7999.905179	13.209664	-0.115131	4.817414
593.958182	7999.908033	13.214669	-0.115154	4.817414
593.854667	7999.891704	13.219674	-0.115134	4.817410
593.816725	7999.913309	13.224679	-0.115127	4.817416
593.659847	7999.888793	13.229683	-0.115098	4.817410
593.624955	7999.892493	13.234688	-0.115092	4.817411
593.921708	7999.888467	13.239693	-0.115147	4.817409
594.029618	7999.885849	13.244698	-0.115167	4.817407
593.843774	7999.948539	13.249703	-0.115132	4.817427
593.874391	7999.918372	13.254707	-0.115138	4.817418
594.144700	7999.909729	13.259712	-0.115188	4.817414
593.945400	7999.939486	13.264717	-0.115151	4.817423
593.458711	7999.952287	13.269722	-0.115060	4.817429
593.323538	7999.984056	13.274727	-0.115035	4.817439
593.403645	8000.035929	13.279731	-0.115050	4.817454
593.615403	7999.929272	13.284736	-0.115089	4.817422
593.558524	7999.942147	13.289741	-0.115079	4.817426
593.945620	7999.889842	13.294746	-0.115151	4.817409
593.938051	7999.901341	13.299751	-0.115149	4.817412
594.024183	7999.863554	13.304755	-0.115165	4.817401
593.855934	7999.884271	13.309760	-0.115134	4.817408
593.935454	7999.954086	13.314765	-0.115149	4.817428
593.815869	7999.918511	13.319770	-0.115126	4.817418
594.137826	7999.899023	13.324775	-0.115186	4.817411
594.048611	7999.869181	13.329779	-0.115170	4.817402
593.905612	7999.891330	13.334784	-0.115143	4.817409
594.302496	7999.871904	13.339789	-0.115217	4.817402
594.084610	7999.867596	13.344794	-0.115176	4.817402
594.014803	7999.921457	13.349799	-0.115163	4.817418
593.682181	7999.898544	13.354803	-0.115101	4.817413
594.076436	7999.911811	13.359808	-0.115175	4.817415
594.485289	7999.915793	13.364813	-0.115251	4.817414
594.351375	7999.887395	13.369818	-0.115226	4.817406
594.256940	7999.881760	13.374823	-0.115208	4.817405
594.100782	7999.891043	13.379827	-0.115179	4.817409
594.217818	7999.855829	13.384832	-0.115201	4.817398
594.254748	7999.878550	13.389837	-0.115207	4.817404
594.366123	7999.859089	13.394842	-0.115228	4.817398
594.303352	7999.923615	13.399847	-0.115216	4.817417
594.113353	7999.900716	13.404851	-0.115181	4.817411
594.532621	7999.878457	13.409856	-0.115259	4.817403
594.614436	7999.891288	13.414861	-0.115274	4.817406
594.367540	7999.836920	13.419866	-0.115228	4.817391
594.237544	7999.886716	13.424871	-0.115204	4.817407
594.433513	7999.874853	13.429875	-0.115240	4.817402
594.587523	7999.875035	13.434880	-0.115269	4.817402
594.335177	7999.895554	13.439885	-0.115222	4.817409
594.277593	7999.870406	13.444890	-0.115211	4.817402
594.579778	7999.901307	13.449895	-0.115267	4.817409
594.325639	7999.895401	13.454899	-0.115220	4.817409
594.351368	7999.854602	13.459904	-0.115225	4.817397
594.571172	7999.919119	13.464909	-0.115266	4.817415
594.045340	7999.888044	13.469914	-0.115168	4.817408
593.932391	7999.887412	13.474919	-0.115147	4.817408
594.011812	7999.925549	13.479923	-0.115162	4.817419
593.922537	7999.897817	13.484928	-0.115145	4.817411
594.054527	7999.901893	13.489933	-0.115169	4.817412
593.976578	7999.901784	13.494938	-0.115155	4.817412
594.019857	7999.921431	13.499943	-0.115163	4.817418
594.407361	7999.857518	13.504947	-0.115235	4.817397
593.958963	7999.903623	13.509952	-0.115151	4.817413
593.968118	7999.972388	13.514957	-0.115153	4.817433
593.824169	7999.921668	13.519962	-0.115126	4.817419
593.475413	7999.972426	13.524967	-0.115061	4.817435
593.877177	7999.950960	13.529971	-0.115136	4.817427
593.759815	7999.923866	13.534976	-0.115114	4.817420
594.263399	7999.883857	13.539981	-0.115208	4.817406
593.971432	7999.892170	13.544986	-0.115153	4.817409
594.035942	7999.908967	13.549991	-0.115165	4.817414
593.916436	7999.880785	13.554995	-0.115143	4.817406
593.535136	7999.933169	13.560000	-0.115072	4.817423
593.609099	7999.943772	13.565005	-0.115086	4.817426
593.260256	7999.959685	13.570010	-0.115021	4.817433
593.000258	7999.995928	13.575015	-0.114972	4.817444
593.456789	7999.985837	13.580019	-0.115057	4.817439
593.443708	7999.985639	13.585024	-0.115055	4.817439
593.534540	7999.952146	13.590029	-0.115072	4.817429
592.998090	7999.990603	13.595034	-0.114972	4.817443
592.929587	8000.001193	13.600039	-0.114959	4.817446
593.269812	8000.016820	13.605043	-0.115022	4.817449
593.164080	7999.945554	13.610048	-0.115003	4.817429
593.603801	7999.947882	13.615053	-0.115084	4.817428
593.740250	7999.920349	13.620058	-0.115110	4.817419
593.891942	7999.894099	13.625063	-0.115138	4.817410
593.508574	7999.983408	13.630067	-0.115067	4.817438
593.443718	7999.940203	13.635072	-0.115054	4.817426
593.298495	8000.028839	13.640077	-0.115027	4.817453
592.975450	8000.009238	13.645082	-0.114967	4.817448
593.720112	7999.953816	13.650087	-0.115106	4.817429
593.708922	7999.996937	13.655091	-0.115104	4.817442
593.476885	7999.978692	13.660096	-0.115060	4.817437
593.657098	8000.037337	13.665101	-0.115094	4.817454
593.676875	7999.960549	13.670106	-0.115098	4.817431
593.751802	7999.920484	13.675111	-0.115111	4.817419
593.961140	7999.936273	13.680115	-0.115150	4.817423
593.567878	7999.963138	13.685120	-0.115077	4.817432
593.909166	7999.959776	13.690125	-0.115141	4.817430
593.799685	7999.926464	13.695130	-0.115120	4.817420
593.904796	7999.930140	13.700135	-0.115140	4.817421
594.301321	7999.908597	13.705139	-0.115214	4.817413
593.970537	7999.899437	13.710144	-0.115152	4.817412
594.040594	7999.903646	13.715149	-0.115165	4.817413
593.715878	7999.927309	13.720154	-0.115104	4.817421
593.977533	7999.905866	13.725159	-0.115153	4.817414
593.769881	7999.956616	13.730163	-0.115114	4.817429
593.756585	7999.927906	13.735168	-0.115112	4.817421
593.953518	7999.969907	13.740173	-0.115148	4.817433
593.421123	7999.972524	13.745178	-0.115049	4.817436
593.684261	7999.946879	13.750183	-0.115098	4.817427
593.975501	7999.945939	13.755187	-0.115152	4.817425
594.037421	7999.939468	13.760192	-0.115164	4.817423
593.797741	7999.979182	13.765197	-0.115119	4.817436
593.957704	7999.955167	13.770202	-0.115149	4.817428
593.877614	7999.952913	13.775207	-0.115134	4.817428
593.745535	7999.983673	13.780211	-0.115109	4.817438
593.743406	7999.953017	13.785216	-0.115109	4.817428
593.278203	7999.979865	13.790221	-0.115022	4.817438
593.604597	7999.905538	13.795226	-0.115083	4.817415
593.682015	7999.917248	13.800231	-0.115097	4.817418
594.086963	7999.884215	13.805235	-0.115173	4.817407
593.950798	7999.914913	13.810240	-0.115147	4.817416
593.920939	7999.917632	13.815245	-0.115142	4.817417
593.667780	7999.901184	13.820250	-0.115095	4.817414
594.084994	7999.896842	13.825255	-0.115172	4.817410
593.849693	7999.942957	13.830259	-0.115128	4.817425
593.920773	7999.909169	13.835264	-0.115142	4.817415
594.022359	7999.902234	13.840269	-0.115160	4.817412
594.193242	7999.886828	13.845274	-0.115192	4.817407
593.961100	7999.928766	13.850279	-0.115149	4.817420
593.873118	7999.950680	13.855283	-0.115133	4.817427
593.502574	7999.938817	13.860288	-0.115063	4.817425
593.486582	7999.961804	13.865293	-0.115060	4.817432
593.683647	7999.951013	13.870298	-0.115097	4.817428
593.296545	7999.969523	13.875303	-0.115025	4.817435
593.584778	7999.989655	13.880307	-0.115079	4.817440
593.520632	7999.938013	13.885312	-0.115067	4.817425
593.410667	8000.043014	13.890317	-0.115046	4.817457
593.478290	7999.948990	13.895322	-0.115059	4.817428
593.284687	7999.997838	13.900327	-0.115023	4.817444
593.575719	8000.011676	13.905331	-0.115077	4.817447
593.741697	7999.945516	13.910336	-0.115108	4.817426
593.806006	7999.960198	13.915341	-0.115120	4.817430
593.484644	7999.938509	13.920346	-0.115060	4.817425
594.104816	7999.897071	13.925351	-0.115175	4.817410
594.218565	7999.917769	13.930355	-0.115196	4.817416
594.482930	7999.885809	13.935360	-0.115245	4.817405
594.306991	7999.918026	13.940365	-0.115213	4.817416
594.422807	7999.872234	13.945370	-0.115234	4.817402
594.598748	7999.893861	13.950375	-0.115267	4.817407
594.362150	7999.891385	13.955379	-0.115223	4.817408
593.867700	7999.906182	13.960384	-0.115131	4.817414
593.992306	7999.923875	13.965389	-0.115154	4.817419
594.373931	7999.863042	13.970394	-0.115225	4.817399
594.142336	7999.928217	13.975399	-0.115182	4.817419
594.336217	7999.914211	13.980403	-0.115218	4.817414
594.369794	7999.891479	13.985408	-0.115224	4.817408
594.627771	7999.948118	13.990413	-0.115272	4.817423
593.552199	8000.004930	13.995418	-0.115072	4.817445
594.253182	7999.914015	14.000423	-0.115202	4.817415
594.652540	7999.891459	14.005427	-0.115276	4.817406
594.514967	7999.890459	14.010432	-0.115251	4.817407
594.266502	7999.909980	14.015437	-0.115204	4.817414
594.667812	7999.853664	14.020442	-0.115279	4.817395
594.373777	7999.884120	14.025447	-0.115224	4.817405
594.606322	7999.886529	14.030451	-0.115268	4.817405
594.505355	7999.845952	14.035456	-0.115249	4.817394
594.569626	7999.871192	14.040461	-0.115261	4.817401
594.656245	7999.858754	14.045466	-0.115277	4.817397
594.612642	7999.896113	14.050471	-0.115269	4.817408
594.651000	7999.914632	14.055475	-0.115276	4.817413
594.692833	7999.868793	14.060480	-0.115283	4.817399
594.749152	7999.905530	14.065485	-0.115294	4.817410
594.544232	7999.879241	14.070490	-0.115256	4.817403
594.883912	7999.901198	14.075495	-0.115319	4.817408
594.446804	7999.940078	14.080499	-0.115237	4.817422
594.281569	7999.908046	14.085504	-0.115207	4.817413
594.818986	7999.917114	14.090509	-0.115307	4.817413
594.640903	7999.873274	14.095514	-0.115273	4.817401
594.248835	7999.903324	14.100519	-0.115200	4.817412
594.544525	7999.903507	14.105523	-0.115255	4.817410
594.332784	7999.895066	14.110528	-0.115216	4.817409
594.377774	7999.920019	14.115533	-0.115224	4.817416
594.476816	7999.861307	14.120538	-0.115243	4.817398
594.393685	7999.889629	14.125543	-0.115227	4.817407
594.731147	7999.871429	14.130547	-0.115290	4.817400
594.497688	7999.855273	14.135552	-0.115246	4.817396
594.821586	7999.880162	14.140557	-0.115307	4.817402
595.033681	7999.856925	14.145562	-0.115346	4.817394
594.746206	7999.884311	14.150567	-0.115293	4.817404
594.858350	7999.899707	14.155571	-0.115313	4.817408
594.377626	7999.885142	14.160576	-0.115224	4.817406
594.334449	7999.920395	14.165581	-0.115216	4.817416
594.121037	7999.970003	14.170586	-0.115176	4.817432
593.913050	7999.966898	14.175591	-0.115137	4.817432
594.057550	7999.974329	14.180595	-0.115164	4.817433
593.543834	7999.984615	14.185600	-0.115068	4.817439
594.603879	7999.957130	14.190605	-0.115266	4.817426
594.588437	7999.897766	14.195610	-0.115263	4.817409
594.121209	7999.919303	14.200615	-0.115176	4.817417
594.236109	7999.895672	14.205619	-0.115197	4.817409
594.253361	7999.926547	14.210624	-0.115200	4.817418
594.119710	7999.942500	14.215629	-0.115175	4.817424
594.515501	7999.891382	14.220634	-0.115249	4.817407
594.632542	7999.884677	14.225639	-0.115271	4.817404
594.461293	7999.924355	14.230643	-0.115239	4.817417
594.169743	7999.888327	14.235648	-0.115185	4.817408
594.393534	7999.891661	14.240653	-0.115226	4.817408
594.452629	7999.898874	14.245658	-0.115237	4.817409
594.381723	7999.907316	14.250663	-0.115224	4.817412
594.467659	7999.940271	14.255667	-0.115240	4.817422
594.815107	7999.853587	14.260672	-0.115304	4.817394
594.727833	7999.882903	14.265677	-0.115288	4.817404
594.696623	7999.882434	14.270682	-0.115282	4.817404
594.859827	7999.860580	14.275687	-0.115313	4.817396
594.906808	7999.885563	14.280691	-0.115321	4.817404
594.695238	7999.843336	14.285696	-0.115282	4.817392
594.760160	7999.877033	14.290701	-0.115294	4.817402
594.439006	7999.871184	14.295706	-0.115234	4.817401
594.548365	7999.888650	14.300711	-0.115254	4.817406
594.552252	7999.890816	14.305715	-0.115255	4.817407
594.443273	7999.878629	14.310720	-0.115235	4.817404
594.626867	7999.884531	14.315725	-0.115269	4.817404
594.572166	7999.888992	14.320730	-0.115259	4.817406
594.871444	7999.867055	14.325735	-0.115314	4.817398
595.076377	7999.869052	14.330739	-0.115353	4.817398
594.971321	7999.859035	14.335744	-0.115333	4.817395
595.060513	7999.875144	14.340749	-0.115349	4.817400
595.159279	7999.835434	14.345754	-0.115368	4.817388
594.911335	7999.870801	14.350759	-0.115322	4.817399
594.883175	7999.867209	14.355763	-0.115316	4.817398
595.046043	7999.357531	14.360768	-0.115346	4.817247

594.951557	7996.057923	14.365773	-0.115327	4.816271
594.698640	7990.642771	14.370778	-0.115276	4.814671
594.890200	7984.031255	14.375783	-0.115307	4.812714
594.875746	7976.758294	14.380787	-0.115300	4.810561
594.741102	7969.108544	14.385792	-0.115270	4.808296
594.819870	7961.324286	14.390797	-0.115279	4.805989
594.832202	7953.449122	14.395802	-0.115276	4.803654
594.560224	7945.530777	14.400807	-0.115220	4.801307
594.771479	7937.498777	14.405811	-0.115254	4.798923
594.766251	7929.565610	14.410816	-0.115248	4.796567
594.521038	7921.530249	14.415821	-0.115197	4.794181
594.397424	7913.603475	14.420826	-0.115169	4.791826
594.529435	7905.487579	14.425831	-0.115188	4.789413
594.862558	7897.547157	14.430835	-0.115245	4.787049
594.645098	7889.456983	14.435840	-0.115199	4.784642
594.498025	7881.570971	14.440845	-0.115167	4.782294
594.587307	7873.521978	14.445850	-0.115178	4.779896
594.436815	7865.534938	14.450855	-0.115145	4.777516
594.391712	7857.497682	14.455859	-0.115131	4.775119
594.384760	7849.518268	14.460864	-0.115125	4.772738
594.105518	7841.534604	14.465869	-0.115067	4.770356
594.255383	7833.497010	14.470874	-0.115090	4.767955
594.387581	7825.462183	14.475879	-0.115109	4.765553
594.284434	7817.511370	14.480883	-0.115085	4.763177
594.005664	7809.512681	14.485888	-0.115028	4.760785
594.293293	7801.486301	14.490893	-0.115076	4.758382
593.942974	7793.525311	14.495898	-0.115006	4.755999
593.821651	7785.452949	14.500903	-0.114978	4.753581
593.979136	7777.529020	14.505907	-0.115002	4.751206
593.669478	7769.432919	14.510912	-0.114939	4.748778
593.253329	7761.477428	14.515917	-0.114856	4.746393
593.760621	7753.386707	14.520922	-0.114945	4.743962
593.702575	7745.439458	14.525927	-0.114929	4.741576
593.796433	7737.415483	14.530931	-0.114941	4.739164
593.316303	7729.491475	14.535936	-0.114847	4.736783
593.192287	7721.425131	14.540941	-0.114818	4.734357
593.524202	7713.425717	14.545946	-0.114875	4.731949
593.429358	7705.348168	14.550951	-0.114852	4.729517
593.456791	7697.424931	14.555955	-0.114852	4.727130
593.340232	7689.368983	14.560960	-0.114825	4.724702
593.512770	7681.440395	14.565965	-0.114852	4.722310
593.393668	7673.437180	14.570970	-0.114824	4.719896
593.366480	7665.445977	14.575975	-0.114814	4.717483
593.433097	7657.435731	14.580979	-0.114821	4.715064
593.195328	7649.444158	14.585984	-0.114772	4.712649
592.927030	7641.417364	14.590989	-0.114717	4.710223
592.952971	7633.456430	14.595994	-0.114716	4.707814
592.733524	7625.424922	14.600999	-0.114670	4.705384
592.785314	7617.488854	14.606003	-0.114674	4.702981
592.427737	7609.460864	14.611008	-0.114603	4.700549
592.473303	7601.521654	14.616013	-0.114606	4.698142
592.768423	7593.421046	14.621018	-0.114655	4.695685
592.401352	7585.410853	14.626023	-0.114582	4.693255
592.783712	7577.400216	14.631027	-0.114648	4.690822
592.672115	7569.393452	14.636032	-0.114622	4.688390
591.968515	7561.483881	14.641037	-0.114486	4.685987
592.131830	7553.391255	14.646042	-0.114511	4.683526
591.944544	7545.452277	14.651047	-0.114471	4.681111
591.821208	7537.491052	14.656051	-0.114442	4.678687
592.005745	7529.442847	14.661056	-0.114471	4.676236
591.962493	7521.385760	14.666061	-0.114458	4.673781
591.770915	7513.385707	14.671066	-0.114417	4.671342
591.663813	7505.307283	14.676071	-0.114392	4.668878
591.813975	7497.394423	14.681075	-0.114415	4.666462
591.818919	7489.324774	14.686080	-0.114410	4.663998
591.111211	7481.511101	14.691085	-0.114273	4.661612
591.329097	7473.381021	14.696090	-0.114309	4.659126
591.238657	7465.392377	14.701095	-0.114287	4.656683
591.566987	7457.339335	14.706099	-0.114342	4.654218
591.753407	7449.381971	14.711104	-0.114372	4.651782
591.653333	7441.376365	14.716109	-0.114348	4.649330
591.601378	7433.440259	14.721114	-0.114333	4.646897
591.354918	7425.326983	14.726119	-0.114282	4.644409
591.655607	7417.461699	14.731123	-0.114333	4.641996
591.460512	7409.388636	14.736128	-0.114291	4.639518
591.238557	7401.444953	14.741133	-0.114244	4.637078
591.288240	7393.362387	14.746138	-0.114248	4.634594
591.258790	7385.403926	14.751143	-0.114238	4.632147
591.081530	7377.400009	14.756147	-0.114199	4.629685
591.075912	7369.368923	14.761152	-0.114193	4.627213
591.207559	7361.311652	14.766157	-0.114212	4.624731
591.078507	7353.411823	14.771162	-0.114183	4.622297
590.824932	7345.355369	14.776167	-0.114131	4.619813
591.155474	7337.403844	14.781171	-0.114187	4.617361
591.241832	7329.322258	14.786176	-0.114198	4.614866
591.023519	7321.370831	14.791181	-0.114152	4.612411
591.176047	7313.321043	14.796186	-0.114175	4.609924
591.113664	7305.325444	14.801191	-0.114158	4.607452
591.301934	7297.303353	14.806195	-0.114188	4.604971
591.149466	7289.372053	14.811200	-0.114154	4.602517
591.015364	7281.417787	14.816205	-0.114124	4.600054
590.719379	7273.442090	14.821210	-0.114064	4.597583
590.886101	7265.304308	14.826215	-0.114089	4.595060
590.441608	7257.378156	14.831219	-0.114001	4.592602
590.458828	7249.304017	14.836224	-0.113999	4.590096
590.373615	7241.319093	14.841229	-0.113978	4.587617
590.391575	7233.318050	14.846234	-0.113976	4.585132
590.021370	7225.349978	14.851239	-0.113902	4.582655
590.096316	7217.310269	14.856243	-0.113911	4.580155
589.757214	7209.362976	14.861248	-0.113842	4.577681
590.184188	7201.285341	14.866253	-0.113917	4.575167
590.082204	7193.331702	14.871258	-0.113892	4.572690
589.877803	7185.282778	14.876263	-0.113849	4.570181
589.941604	7177.343095	14.881267	-0.113856	4.567705
590.115990	7169.261064	14.886272	-0.113883	4.565184
589.741920	7161.319413	14.891277	-0.113808	4.562704
589.416756	7153.356975	14.896282	-0.113742	4.560216
589.328879	7145.354683	14.901287	-0.113721	4.557715
589.738595	7137.282945	14.906291	-0.113792	4.555192
589.442151	7129.318703	14.911296	-0.113731	4.552700
589.254619	7121.300415	14.916301	-0.113691	4.550189
589.416772	7113.330153	14.921306	-0.113716	4.547693
588.803678	7105.295808	14.926311	-0.113597	4.545174
588.631997	7097.344686	14.931315	-0.113559	4.542681
588.803715	7089.246300	14.936320	-0.113586	4.540140
589.115367	7081.242824	14.941325	-0.113639	4.537629
588.951174	7073.248281	14.946330	-0.113603	4.535117
588.974497	7065.256775	14.951335	-0.113602	4.532606
588.254786	7057.324281	14.956339	-0.113463	4.530110
588.624834	7049.268470	14.961344	-0.113526	4.527576
588.778968	7041.208928	14.966349	-0.113550	4.525040
588.864826	7033.285246	14.971354	-0.113561	4.522544
588.407336	7025.254803	14.976359	-0.113470	4.520012
588.163302	7017.376600	14.981363	-0.113420	4.517528
588.509813	7009.249109	14.986368	-0.113479	4.514964
588.549264	7001.245650	14.991373	-0.113481	4.512438
588.473883	6993.206260	14.996378	-0.113462	4.509899
588.548073	6985.187755	15.001383	-0.113470	4.507365
588.125831	6977.266524	15.006387	-0.113386	4.504859
588.043552	6969.251723	15.011392	-0.113366	4.502323
588.394139	6961.157143	15.016397	-0.113426	4.499762
588.546622	6953.195258	15.021402	-0.113449	4.497240
588.483899	6945.116989	15.026407	-0.113432	4.494680
588.661456	6937.236605	15.031411	-0.113460	4.492182
588.221957	6929.215903	15.036416	-0.113373	4.489635
588.108128	6921.203135	15.041421	-0.113346	4.487091
587.896940	6913.192154	15.046426	-0.113302	4.484546
587.897169	6905.256994	15.051431	-0.113296	4.482024
588.227210	6897.164367	15.056435	-0.113352	4.479452
588.142266	6889.177412	15.061440	-0.113331	4.476910
588.032379	6881.206124	15.066445	-0.113306	4.474372
588.178701	6873.252873	15.071450	-0.113328	4.471839
587.737462	6865.175405	15.076455	-0.113240	4.469263
588.065652	6857.162368	15.081459	-0.113296	4.466709
588.045678	6849.130951	15.086464	-0.113287	4.464146
588.073301	6841.183691	15.091469	-0.113287	4.461609
587.959914	6833.179341	15.096474	-0.113261	4.459051
587.842779	6825.167969	15.101479	-0.113234	4.456490
587.861566	6817.170113	15.106483	-0.113232	4.453932
587.585404	6809.234631	15.111488	-0.113175	4.451391
587.672614	6801.133898	15.116493	-0.113186	4.448798
587.545119	6793.178316	15.121498	-0.113157	4.446248
586.809300	6785.192433	15.126503	-0.113015	4.443685
586.838959	6777.232233	15.131507	-0.113015	4.441132
587.077535	6769.148997	15.136512	-0.113054	4.438538
587.154909	6761.178786	15.141517	-0.113063	4.435979
587.610040	6753.095633	15.146522	-0.113143	4.433384
586.790654	6745.167958	15.151527	-0.112985	4.430831
587.085938	6737.140278	15.156531	-0.113035	4.428251
587.155444	6729.082959	15.161536	-0.113042	4.425657
586.762239	6721.114382	15.166541	-0.112964	4.423089
586.694688	6713.187884	15.171546	-0.112946	4.420534
586.957617	6705.093076	15.176551	-0.112990	4.417925
587.077639	6697.048879	15.181555	-0.113007	4.415331
586.776400	6689.137361	15.186560	-0.112946	4.412775
586.713634	6681.086361	15.191565	-0.112929	4.410174
586.145680	6673.209202	15.196570	-0.112818	4.407625
585.773215	6665.168376	15.201575	-0.112743	4.405023
586.121384	6657.225782	15.206579	-0.112803	4.402454
586.406779	6649.119161	15.211584	-0.112851	4.399831
586.236642	6641.086213	15.216589	-0.112814	4.397228
586.572033	6633.051731	15.221594	-0.112871	4.394625
586.238999	6625.137211	15.226599	-0.112804	4.392056
585.855953	6617.125499	15.231603	-0.112727	4.389454
585.760067	6609.120963	15.236608	-0.112704	4.386854
586.104736	6600.995627	15.241613	-0.112763	4.384216
586.060254	6593.110062	15.246618	-0.112749	4.381652
585.890757	6585.058885	15.251623	-0.112712	4.379031
585.911188	6577.160358	15.256627	-0.112711	4.376460
585.786243	6569.119875	15.261632	-0.112682	4.373841
585.737981	6561.101882	15.266637	-0.112668	4.371227
586.061162	6553.112773	15.271642	-0.112723	4.368624
585.465242	6545.127010	15.276647	-0.112607	4.366014
584.835272	6537.243522	15.281651	-0.112484	4.363436
584.833858	6529.268739	15.286656	-0.112479	4.360831
585.413069	6521.139482	15.291661	-0.112581	4.358177
585.316664	6513.193416	15.296666	-0.112558	4.355578
585.209027	6505.133176	15.301671	-0.112533	4.352939
585.152931	6497.077715	15.306675	-0.112517	4.350301
585.063312	6489.124102	15.311680	-0.112495	4.347694
584.515606	6481.120655	15.316685	-0.112388	4.345066
584.963222	6473.148700	15.321690	-0.112466	4.342454
585.594943	6465.016572	15.326695	-0.112578	4.339789
585.458035	6457.130793	15.331699	-0.112548	4.337197
584.903137	6449.190939	15.336704	-0.112439	4.334584
584.919932	6441.178439	15.341709	-0.112437	4.331949
585.129361	6433.129362	15.346714	-0.112471	4.329301
584.567793	6425.194140	15.351719	-0.112361	4.326684
585.048223	6417.113418	15.356723	-0.112445	4.324026
584.610890	6409.327194	15.361728	-0.112359	4.321455
584.903866	6401.120519	15.366733	-0.112408	4.318750
584.623016	6393.206930	15.371738	-0.112350	4.316136
585.242786	6385.106249	15.376743	-0.112460	4.313465
584.858026	6377.239911	15.381747	-0.112384	4.310863
584.636065	6369.163050	15.386752	-0.112337	4.308190
584.638206	6361.085715	15.391757	-0.112332	4.305517
584.645458	6353.149956	15.396762	-0.112328	4.302890
584.780121	6345.054735	15.401767	-0.112348	4.300209
584.636134	6337.155205	15.406771	-0.112316	4.297589
584.378907	6329.124218	15.411776	-0.112263	4.294923
584.119093	6321.143531	15.416781	-0.112209	4.292271
584.006118	6313.141505	15.421786	-0.112183	4.289613
583.920641	6305.171945	15.426791	-0.112162	4.286963
584.041296	6297.081764	15.431795	-0.112179	4.284274
583.971754	6289.170524	15.436800	-0.112161	4.281641
584.249690	6281.069255	15.441805	-0.112207	4.278946
584.390152	6273.173428	15.446810	-0.112228	4.276317
583.912245	6265.228106	15.451815	-0.112134	4.273664
584.253888	6257.113859	15.456819	-0.112192	4.270960
584.397305	6249.062459	15.461824	-0.112214	4.268274
584.435681	6241.021804	15.466829	-0.112215	4.265589
584.426110	6233.147236	15.471834	-0.112208	4.262957
584.373913	6225.085559	15.476839	-0.112193	4.260260
584.273553	6217.206660	15.481843	-0.112170	4.257623
584.300506	6209.106278	15.486848	-0.112169	4.254911
584.291384	6201.103384	15.491853	-0.112162	4.252229
584.443042	6193.092509	15.496858	-0.112185	4.249545
584.208806	6185.019760	15.501863	-0.112136	4.246834
583.591932	6177.122496	15.506867	-0.112016	4.244177
584.020821	6169.186492	15.511872	-0.112091	4.241516
584.004861	6161.145981	15.516877	-0.112083	4.238813
583.785366	6153.217858	15.521882	-0.112037	4.236144
583.534110	6145.157609	15.526887	-0.111985	4.233429
583.793072	6137.102908	15.531891	-0.112028	4.230719
583.411285	6129.150645	15.536896	-0.111951	4.228036
583.555411	6121.091164	15.541901	-0.111973	4.225319
583.778382	6113.139823	15.546906	-0.112009	4.222639
583.788629	6105.066958	15.551911	-0.112006	4.219913
583.860674	6097.152574	15.556915	-0.112014	4.217240
583.911736	6089.095211	15.561920	-0.112018	4.214517
584.075794	6081.059756	15.566925	-0.112043	4.211801
583.408106	6073.159234	15.571930	-0.111914	4.209119
582.762435	6065.210799	15.576935	-0.111788	4.206420
583.204528	6057.110133	15.581939	-0.111865	4.203679
582.799952	6049.186565	15.586944	-0.111785	4.200987
582.826333	6041.130011	15.591949	-0.111784	4.198253
583.104446	6033.097994	15.596954	-0.111831	4.195529
582.864341	6025.040474	15.601959	-0.111781	4.192788
582.867652	6017.062832	15.606963	-0.111776	4.190075
582.760717	6009.101391	15.611968	-0.111751	4.187365
582.718907	6001.006386	15.616973	-0.111738	4.184608
582.685227	5993.133563	15.621978	-0.111727	4.181925
582.823527	5985.032014	15.626983	-0.111747	4.179165
582.732325	5977.096404	15.631987	-0.111725	4.176457
582.242127	5969.114818	15.636992	-0.111628	4.173726
582.251487	5961.040964	15.641997	-0.111625	4.170968
582.418676	5953.083823	15.647002	-0.111651	4.168250
582.432315	5945.014924	15.652007	-0.111648	4.165490
582.207625	5937.133925	15.657011	-0.111601	4.162790
582.509715	5929.092779	15.662016	-0.111652	4.160040
582.186085	5921.126466	15.667021	-0.111586	4.157305
581.889652	5913.129070	15.672026	-0.111526	4.154559
581.754753	5905.163107	15.677031	-0.111496	4.151823
581.205041	5897.163852	15.682035	-0.111388	4.149069
581.199403	5889.168509	15.687040	-0.111382	4.146322
581.441509	5881.049612	15.692045	-0.111421	4.143533
581.331948	5873.164881	15.697050	-0.111396	4.140818
581.349417	5865.079462	15.702055	-0.111394	4.138034
581.537041	5857.107286	15.707059	-0.111423	4.135290
581.445716	5849.117263	15.712064	-0.111401	4.132534
581.558457	5841.012788	15.717069	-0.111417	4.129739
581.535999	5833.122252	15.722074	-0.111408	4.127014
581.530686	5825.033942	15.727079	-0.111401	4.124220
581.373087	5817.206087	15.732083	-0.111367	4.121512
581.184255	5809.140167	15.737088	-0.111326	4.118719
580.701989	5801.167737	15.742093	-0.111231	4.115952
581.125482	5793.111751	15.747098	-0.111305	4.113167
581.495129	5785.050545	15.752103	-0.111368	4.110378
581.547003	5777.090763	15.757107	-0.111373	4.107617
581.481574	5769.096873	15.762112	-0.111355	4.104841
581.340799	5761.148238	15.767117	-0.111324	4.102078
581.699172	5753.059514	15.772122	-0.111385	4.099272
581.349473	5745.130938	15.777127	-0.111315	4.096509
581.544837	5737.088287	15.782131	-0.111346	4.093712
581.252745	5729.153121	15.787136	-0.111286	4.090944
580.923667	5721.171227	15.792141	-0.111220	4.088158
581.434420	5713.049818	15.797146	-0.111310	4.085332
581.526066	5705.119051	15.802151	-0.111322	4.082566
581.004430	5697.182164	15.807155	-0.111219	4.079786
580.912475	5689.207295	15.812160	-0.111197	4.076997
580.563199	5681.172741	15.817165	-0.111127	4.074182
580.089592	5673.211491	15.822170	-0.111033	4.071389
580.143896	5665.126005	15.827175	-0.111038	4.068558
580.701403	5657.074853	15.832179	-0.111136	4.065744
580.610659	5649.098240	15.837184	-0.111114	4.062946
580.659423	5641.053668	15.842189	-0.111118	4.060123
580.750764	5633.105282	15.847194	-0.111130	4.057333
580.485242	5625.063939	15.852199	-0.111075	4.054503
580.583600	5617.116510	15.857203	-0.111088	4.051709
580.735360	5609.121677	15.862208	-0.111111	4.048898
580.378430	5601.163267	15.867213	-0.111040	4.046090
580.803004	5593.127783	15.872218	-0.111113	4.043264
580.736197	5585.093587	15.877223	-0.111096	4.040430
580.650710	5577.172004	15.882227	-0.111075	4.037633
580.720240	5569.122739	15.887232	-0.111082	4.034791
580.532248	5561.086129	15.892237	-0.111042	4.031948
580.618517	5553.119830	15.897242	-0.111053	4.029132
580.462477	5545.086139	15.902247	-0.111018	4.026286
580.256105	5537.121264	15.907251	-0.110975	4.023462
580.450568	5529.096437	15.912256	-0.111006	4.020621
580.202840	5521.121006	15.917261	-0.110954	4.017788
579.866795	5513.198418	15.922266	-0.110887	4.014971
580.056809	5505.187196	15.927271	-0.110917	4.012129
579.969216	5497.163589	15.932275	-0.110895	4.009276
580.095935	5489.152531	15.937280	-0.110913	4.006428
579.773498	5481.099521	15.942285	-0.110848	4.003557
579.741353	5473.177377	15.947290	-0.110837	4.000734
579.568049	5465.180751	15.952295	-0.110799	3.997881
579.323390	5457.196758	15.957299	-0.110749	3.995029
579.966575	5449.112961	15.962304	-0.110863	3.992155
579.934350	5441.093730	15.967309	-0.110852	3.989289
579.711359	5433.206325	15.972314	-0.110805	3.986466
578.961666	5425.202264	15.977319	-0.110660	3.983590
579.133802	5417.194201	15.982323	-0.110687	3.980726
579.374756	5409.179818	15.987328	-0.110727	3.977859
579.007543	5401.180431	15.992333	-0.110653	3.974985
579.031105	5393.225481	15.997338	-0.110652	3.972132
578.798342	5385.180918	16.002343	-0.110604	3.969240
578.631387	5377.226844	16.007347	-0.110567	3.966379
578.867405	5369.140785	16.012352	-0.110606	3.963476
578.853020	5361.174363	16.017357	-0.110598	3.960609
578.860208	5353.242126	16.022362	-0.110594	3.957753
578.434988	5345.243523	16.027367	-0.110510	3.954863
578.851699	5337.164028	16.032371	-0.110582	3.951957
579.276754	5329.140916	16.037376	-0.110656	3.949070
578.974262	5321.153091	16.042381	-0.110594	3.946180
579.000899	5313.158129	16.047386	-0.110594	3.943291
579.201737	5305.123107	16.052391	-0.110626	3.940389
579.170257	5297.175565	16.057395	-0.110615	3.937512
578.502557	5289.263685	16.062400	-0.110485	3.934634
578.328882	5281.208627	16.067405	-0.110448	3.931711
578.956686	5273.103002	16.072410	-0.110559	3.928783
578.643912	5265.193494	16.077415	-0.110496	3.925906
579.105329	5257.140766	16.082419	-0.110577	3.922989
578.964656	5249.237562	16.087424	-0.110545	3.920114
578.416788	5241.265366	16.092429	-0.110438	3.917203
578.039454	5233.298130	16.097434	-0.110362	3.914295
578.208746	5225.249178	16.102439	-0.110389	3.911366
578.036307	5217.200236	16.107443	-0.110351	3.908428
578.022188	5209.202934	16.112448	-0.110343	3.905509
577.961844	5201.193566	16.117453	-0.110327	3.902583
578.005477	5193.237644	16.122458	-0.110330	3.899677
577.819377	5185.244461	16.127463	-0.110290	3.896750
577.970170	5177.226496	16.132467	-0.110313	3.893818
577.944631	5169.258093	16.137472	-0.110303	3.890899
577.674069	5161.219536	16.142477	-0.110247	3.887947
577.632333	5153.223286	16.147482	-0.110234	3.885013
577.360015	5145.311966	16.152487	-0.110178	3.882104
577.440889	5137.270171	16.157491	-0.110188	3.879151
577.202400	5129.349602	16.162496	-0.110138	3.876234
577.681764	5121.139445	16.167501	-0.110222	3.873223
577.775031	5113.074602	16.172506	-0.110234	3.870255
577.982008	5105.082441	16.177511	-0.110267	3.867314
577.764159	5097.102981	16.182515	-0.110222	3.864367
578.082086	5089.208043	16.187520	-0.110276	3.861460
577.984888	5081.189232	16.192525	-0.110252	3.858496
577.797437	5073.252624	16.197530	-0.110212	3.855558
577.408732	5065.300599	16.202535	-0.110135	3.852609
577.297301	5057.246418	16.207539	-0.110109	3.849625
577.632816	5049.251497	16.212544	-0.110166	3.846670
577.468075	5041.218697	16.217549	-0.110130	3.843688
577.656181	5033.318380	16.222554	-0.110160	3.840760
577.343766	5025.291364	16.227559	-0.110096	3.837773
577.455665	5017.232883	16.232563	-0.110112	3.834781
577.376513	5009.327617	16.237568	-0.110092	3.831839
577.255307	5001.311839	16.242573	-0.110064	3.828853
577.181126	4993.288750	16.247578	-0.110045	3.825862
577.402763	4985.254716	16.252583	-0.110081	3.822872
577.229359	4977.271748	16.257587	-0.110043	3.819890
577.342849	4969.312517	16.262592	-0.110059	3.816921
576.655995	4961.348964	16.267597	-0.109926	3.813930
577.025747	4953.287781	16.272602	-0.109990	3.810923
576.592113	4945.327980	16.277607	-0.109904	3.807934
576.823818	4937.246718	16.282611	-0.109942	3.804913
577.167513	4929.309956	16.287616	-0.110000	3.801945
576.889445	4921.305011	16.292621	-0.109943	3.798936
577.131074	4913.307731	16.297626	-0.109983	3.795939
576.653445	4905.387430	16.302631	-0.109889	3.792952
576.675114	4897.314757	16.307635	-0.109888	3.789917
576.650797	4889.326797	16.312640	-0.109878	3.786910
576.627615	4881.253987	16.317645	-0.109868	3.783869
576.248630	4873.369192	16.322650	-0.109793	3.780888
576.300952	4865.341111	16.327655	-0.109797	3.777861
576.315296	4857.310210	16.332659	-0.109794	3.774829
575.977008	4849.399998	16.337664	-0.109726	3.771832
576.080781	4841.327777	16.342669	-0.109740	3.768782
576.114872	4833.358726	16.347674	-0.109741	3.765767
576.037178	4825.351098	16.352679	-0.109722	3.762732
576.179714	4817.356808	16.357683	-0.109743	3.759705
575.737472	4809.476252	16.362688	-0.109655	3.756704
575.469165	4801.407160	16.367693	-0.109600	3.753634
575.499362	4793.413041	16.372698	-0.109600	3.750597
575.104332	4785.441593	16.377703	-0.109522	3.747556
575.182063	4777.369760	16.382707	-0.109531	3.744485
575.397652	4769.431746	16.387712	-0.109566	3.741467
575.163018	4761.397792	16.392717	-0.109517	3.738398
575.304911	4753.377539	16.397722	-0.109538	3.735341
575.392420	4745.386080	16.402727	-0.109549	3.732292
575.124894	4737.363544	16.407731	-0.109494	3.729219
575.051214	4729.421715	16.412736	-0.109475	3.726180
575.051569	4721.405798	16.417741	-0.109470	3.723111
574.808286	4713.477479	16.422746	-0.109419	3.720067
575.058149	4705.492715	16.427751	-0.109461	3.717012
574.895294	4697.415331	16.432755	-0.109425	3.713908
575.174330	4689.388950	16.437760	-0.109472	3.710832
574.956535	4681.394450	16.442765	-0.109426	3.707753
575.012238	4673.403267	16.447770	-0.109431	3.704680
574.573419	4665.487857	16.452775	-0.109344	3.701622
574.986928	4657.380158	16.457779	-0.109416	3.698508
575.215783	4649.379582	16.462784	-0.109453	3.695428
575.076904	4641.397975	16.467789	-0.109422	3.692343
575.423596	4633.383363	16.472794	-0.109481	3.689256
575.294563	4625.433046	16.477799	-0.109452	3.686179
575.126355	4617.417876	16.482803	-0.109415	3.683072
575.197507	4609.473976	16.487808	-0.109423	3.679998
575.061813	4601.480643	16.492813	-0.109393	3.676896
574.958922	4593.501548	16.497818	-0.109369	3.673797
574.831964	4585.497119	16.502823	-0.109340	3.670686
574.805575	4577.502313	16.507827	-0.109329	3.667578
574.501441	4569.519668	16.512832	-0.109268	3.664465
574.587699	4561.496314	16.517837	-0.109278	3.661344
574.403501	4553.558454	16.522842	-0.109239	3.658247
574.571953	4545.495031	16.527847	-0.109265	3.655107
574.490317	4537.506148	16.532851	-0.109244	3.651987
574.333245	4529.527774	16.537856	-0.109210	3.648866
574.510279	4521.527461	16.542861	-0.109238	3.645743
574.533688	4513.556615	16.547866	-0.109237	3.642625
574.456998	4505.516722	16.552871	-0.109217	3.639474
574.494304	4497.572167	16.557875	-0.109219	3.636361
574.385708	4489.576261	16.562880	-0.109193	3.633221
573.889909	4481.593185	16.567885	-0.109096	3.630073
573.331952	4473.689160	16.572890	-0.108987	3.626951
573.400967	4465.622353	16.577895	-0.108994	3.623780
573.352639	4457.578065	16.582899	-0.108980	3.620612
573.378064	4449.614784	16.587904	-0.108980	3.617475
573.692637	4441.495284	16.592909	-0.109033	3.614282
573.631019	4433.580582	16.597914	-0.109016	3.611156
573.488357	4425.586962	16.602919	-0.108984	3.607994
573.537817	4417.553417	16.607923	-0.108988	3.604819
573.462590	4409.649499	16.612928	-0.108969	3.601689
572.712687	4401.720263	16.617933	-0.108824	3.598527
573.318479	4393.616341	16.622938	-0.108932	3.595331
573.359118	4385.647849	16.627943	-0.108934	3.592171
572.958416	4377.665184	16.632947	-0.108854	3.588989
572.704499	4369.691589	16.637952	-0.108802	3.585812
573.118100	4361.602404	16.642957	-0.108873	3.582605
572.852048	4353.637745	16.647962	-0.108819	3.579426
572.825385	4345.661040	16.652967	-0.108808	3.576246
572.184795	4337.743175	16.657971	-0.108684	3.573068
572.364233	4329.714703	16.662976	-0.108712	3.569868
572.183509	4321.712362	16.667981	-0.108673	3.566665
571.840368	4313.736444	16.672986	-0.108604	3.563464
571.608288	4305.781365	16.677991	-0.108556	3.560272
571.662319	4297.773906	16.682995	-0.108560	3.557065
571.701951	4289.718715	16.688000	-0.108562	3.553835
571.709602	4281.624277	16.693005	-0.108559	3.550586
572.053806	4273.616641	16.698010	-0.108617	3.547378
572.096392	4265.600943	16.703015	-0.108620	3.544156
572.014163	4257.661699	16.708019	-0.108600	3.540957
572.204984	4249.704218	16.713024	-0.108630	3.537757
572.127266	4241.673777	16.718029	-0.108610	3.534516
571.988541	4233.707985	16.723034	-0.108579	3.531296
571.844303	4225.730641	16.728039	-0.108547	3.528069
571.583497	4217.734145	16.733043	-0.108493	3.524827
571.479257	4209.810914	16.738048	-0.108469	3.521617
571.543035	4201.773359	16.743053	-0.108475	3.518362
571.615315	4193.791807	16.748058	-0.108483	3.515128
571.404784	4185.802660	16.753063	-0.108439	3.511878
571.066732	4177.824803	16.758067	-0.108371	3.508627
571.314954	4169.814832	16.763072	-0.108412	3.505377
570.966930	4161.871918	16.768077	-0.108342	3.502133
571.445040	4153.765187	16.773082	-0.108425	3.498846
571.040873	4145.844744	16.778087	-0.108345	3.495603
571.187909	4137.792012	16.783091	-0.108367	3.492321
570.871803	4129.831548	16.788096	-0.108303	3.489058
571.028028	4121.833591	16.793101	-0.108327	3.485792
570.954441	4113.835412	16.798106	-0.108308	3.482516
571.217155	4105.786770	16.803111	-0.108351	3.479227
571.002093	4097.864449	16.808115	-0.108306	3.475971
571.210498	4089.853407	16.813120	-0.108340	3.472690
570.890716	4081.850473	16.818125	-0.108275	3.469391
571.018154	4073.873190	16.823130	-0.108293	3.466115
570.905271	4065.889426	16.828135	-0.108267	3.462824
570.305814	4058.001120	16.833139	-0.108150	3.459554
570.160103	4050.010388	16.838144	-0.108118	3.456253
570.062060	4041.933543	16.843149	-0.108094	3.452916
570.258735	4033.890394	16.848154	-0.108126	3.449598
570.517561	4025.889805	16.853159	-0.108169	3.446298
570.509219	4017.888480	16.858163	-0.108162	3.442985
570.412582	4009.948791	16.863168	-0.108139	3.439691
570.741194	4001.920112	16.868173	-0.108195	3.436372
570.887159	3993.889293	16.873178	-0.108216	3.433042
571.028564	3985.918384	16.878183	-0.108238	3.429734
570.815765	3978.008431	16.883187	-0.108193	3.426436
570.790631	3969.999205	16.888192	-0.108183	3.423100
570.393214	3962.036258	16.893197	-0.108104	3.419767
570.357040	3954.052641	16.898202	-0.108092	3.416434
570.532250	3945.989687	16.903207	-0.108119	3.413073
570.682877	3937.944122	16.908211	-0.108142	3.409715
570.915258	3929.968900	16.913216	-0.108180	3.406385
570.602427	3922.030863	16.918221	-0.108116	3.403049
570.607482	3914.064275	16.923226	-0.108112	3.399709
570.310209	3906.142229	16.928231	-0.108051	3.396373
570.371631	3898.029117	16.933235	-0.108057	3.392967
570.304207	3890.036723	16.938240	-0.108040	3.389603
570.400945	3881.998297	16.943245	-0.108052	3.386223
570.183729	3874.062770	16.948250	-0.108007	3.382871
570.177159	3866.109064	16.953255	-0.108000	3.379516
570.027528	3858.115664	16.958259	-0.107967	3.376135
570.064504	3850.115794	16.963264	-0.107969	3.372755
570.097690	3842.060826	16.968269	-0.107970	3.369349
570.204968	3834.065072	16.973274	-0.107984	3.365966
570.804531	3826.019279	16.978279	-0.108091	3.362577
570.618854	3818.084672	16.983283	-0.108051	3.359203
570.203856	3810.234611	16.988288	-0.107969	3.355853
569.749151	3802.247075	16.993293	-0.107879	3.352440
569.859760	3794.212707	16.998298	-0.107894	3.349024
569.837352	3786.233271	17.003303	-0.107885	3.345624
569.316029	3778.266915	17.008307	-0.107782	3.342206
569.545635	3770.261272	17.013312	-0.107820	3.338797
569.874797	3762.195071	17.018317	-0.107876	3.335362
569.502485	3754.260178	17.023322	-0.107801	3.331953
569.807154	3746.200872	17.028327	-0.107853	3.328513
569.756771	3738.219792	17.033331	-0.107838	3.325089
569.699575	3730.299190	17.038336	-0.107822	3.321688
569.312339	3722.316596	17.043341	-0.107745	3.318243
569.416440	3714.315346	17.048346	-0.107759	3.314806
569.452451	3706.306690	17.053351	-0.107760	3.311360
569.468085	3698.251707	17.058355	-0.107758	3.307889
569.577453	3690.257517	17.063360	-0.107773	3.304445
569.385927	3682.317472	17.068365	-0.107732	3.301008
569.530585	3674.300623	17.073370	-0.107754	3.297548
569.640514	3666.311124	17.078375	-0.107769	3.294095
569.407392	3658.368940	17.083379	-0.107720	3.290645
569.246676	3650.368911	17.088384	-0.107685	3.287169
569.174764	3642.341318	17.093389	-0.107667	3.283682
568.991179	3634.422937	17.098394	-0.107627	3.280233
569.095286	3626.435062	17.103399	-0.107641	3.276762
569.075773	3618.406734	17.108403	-0.107632	3.273265
569.033320	3610.420594	17.113408	-0.107619	3.269781
568.851469	3602.440787	17.118413	-0.107580	3.266291
569.077169	3594.413498	17.123418	-0.107617	3.262793
569.132368	3586.416869	17.128423	-0.107622	3.259297
568.948306	3578.485130	17.133427	-0.107582	3.255817
568.765826	3570.520531	17.138432	-0.107543	3.252318
568.740032	3562.475377	17.143437	-0.107533	3.248787
568.239534	3554.576930	17.148442	-0.107435	3.245297
568.359972	3546.578938	17.153447	-0.107452	3.241785
568.081244	3538.582919	17.158451	-0.107395	3.238253
568.299287	3530.557736	17.163456	-0.107430	3.234725
567.993086	3522.611620	17.168461	-0.107368	3.231207
568.086107	3514.572482	17.173466	-0.107380	3.227660
568.154272	3506.538836	17.178471	-0.107387	3.224111
568.349774	3498.546391	17.183475	-0.107419	3.220581
567.937671	3490.632783	17.188480	-0.107337	3.217057
567.464220	3482.641731	17.193485	-0.107243	3.213492
567.753677	3474.602052	17.198490	-0.107292	3.209933
567.701770	3466.637335	17.203495	-0.107277	3.206390
567.900234	3458.562230	17.208499	-0.107309	3.202804
567.677425	3450.637876	17.213504	-0.107262	3.199263
567.490350	3442.698701	17.218509	-0.107222	3.195713
567.734391	3434.655801	17.223514	-0.107262	3.192132
567.714863	3426.661814	17.228519	-0.107253	3.188557
568.145515	3418.581140	17.233523	-0.107328	3.184958
568.340283	3410.663770	17.238528	-0.107359	3.181419
567.954663	3402.698594	17.243533	-0.107282	3.177829
567.380115	3394.789414	17.248538	-0.107170	3.174252
567.796348	3386.741840	17.253543	-0.107242	3.170652
567.718970	3378.763725	17.258547	-0.107222	3.167057
567.522147	3370.795282	17.263552	-0.107180	3.163457
567.368601	3362.827630	17.268557	-0.107147	3.159856
567.251335	3354.838649	17.273562	-0.107120	3.156242
567.332010	3346.838770	17.278567	-0.107129	3.152628
566.699167	3338.922993	17.283571	-0.107006	3.149016
567.325075	3330.805204	17.288576	-0.107118	3.145365
566.990669	3322.878633	17.293581	-0.107050	3.141753
566.813033	3314.892273	17.298586	-0.107012	3.138117
567.060649	3306.875872	17.303591	-0.107053	3.134482
566.752282	3298.934807	17.308595	-0.106990	3.130852
566.397809	3290.948152	17.313600	-0.106919	3.127195
566.479511	3282.939171	17.318605	-0.106929	3.123543
566.707201	3274.926989	17.323610	-0.106966	3.119892
566.311894	3267.049831	17.328615	-0.106887	3.116270
566.113074	3259.023369	17.333619	-0.106845	3.112585
566.510739	3250.951369	17.338624	-0.106913	3.108901
566.257330	3242.997071	17.343629	-0.106861	3.105238
566.077660	3235.038068	17.348634	-0.106822	3.101571
566.359720	3227.031079	17.353639	-0.106870	3.097899
566.144555	3219.048556	17.358643	-0.106824	3.094211
566.224611	3211.060603	17.363648	-0.106834	3.090530
566.022797	3203.081044	17.368653	-0.106791	3.086835
566.187508	3195.068435	17.373658	-0.106817	3.083137
566.247232	3187.096282	17.378663	-0.106822	3.079449
565.860678	3179.143578	17.383667	-0.106745	3.075745
565.727632	3171.172012	17.388672	-0.106715	3.072039
565.626172	3163.128330	17.393677	-0.106691	3.068297
565.243052	3155.182481	17.398682	-0.106614	3.064582
565.470987	3147.190249	17.403687	-0.106652	3.060870
565.507919	3139.173107	17.408691	-0.106653	3.057133
565.696689	3131.172779	17.413696	-0.106683	3.053407
565.469005	3123.189203	17.418701	-0.106636	3.049663
565.204665	3115.259346	17.423706	-0.106581	3.045939
565.539936	3107.229074	17.428711	-0.106638	3.042192
565.604871	3099.205421	17.433715	-0.106645	3.038430
565.912991	3091.222756	17.438720	-0.106697	3.034695
565.315283	3083.343764	17.443725	-0.106581	3.030959
565.111998	3075.350026	17.448730	-0.106538	3.027185
564.904738	3067.414422	17.453735	-0.106494	3.023432
565.095739	3059.345820	17.458739	-0.106524	3.019632
564.987028	3051.412550	17.463744	-0.106499	3.015876
564.676177	3043.447921	17.468749	-0.106436	3.012091
564.919313	3035.394111	17.473754	-0.106475	3.008286
564.567296	3027.454136	17.478759	-0.106405	3.004501
564.461869	3019.466023	17.483763	-0.106380	3.000700
565.092110	3011.412543	17.488768	-0.106492	2.996901
564.756261	3003.478991	17.493773	-0.106424	2.993105
564.292256	2995.528789	17.498778	-0.106333	2.989289
564.284507	2987.537624	17.503783	-0.106326	2.985472
564.219607	2979.542574	17.508787	-0.106309	2.981646
564.237635	2971.567177	17.513792	-0.106307	2.977829
563.788350	2963.617702	17.518797	-0.106218	2.973994
563.802324	2955.587918	17.523802	-0.106215	2.970141
564.046846	2947.587187	17.528807	-0.106255	2.966308
563.938813	2939.595199	17.533811	-0.106230	2.962456
563.842216	2931.644151	17.538816	-0.106207	2.958619
563.935302	2923.631183	17.543821	-0.106219	2.954758
563.328175	2915.778285	17.548826	-0.106101	2.950932
563.343077	2907.752795	17.553831	-0.106098	2.947050
563.354393	2899.733756	17.558835	-0.106095	2.943166
563.401344	2891.743276	17.563840	-0.106098	2.939292
562.643667	2883.879558	17.568845	-0.105952	2.935432
562.876832	2875.815403	17.573850	-0.105990	2.931523
562.751186	2867.840336	17.578855	-0.105962	2.927632
562.575417	2859.859698	17.583859	-0.105924	2.923731
562.747172	2851.840671	17.588864	-0.105950	2.919824
562.838958	2843.869820	17.593869	-0.105962	2.915932
563.058062	2835.780796	17.598874	-0.105998	2.911983
562.752265	2827.839010	17.603879	-0.105936	2.908073
562.690296	2819.814938	17.608883	-0.105919	2.904130
562.909972	2811.877123	17.613888	-0.105955	2.900240
562.977115	2803.866047	17.618893	-0.105962	2.896300
563.129645	2795.845557	17.623898	-0.105985	2.892354
563.267346	2787.870452	17.628903	-0.106005	2.888425
562.754253	2779.977668	17.633907	-0.105905	2.884496
563.032297	2771.995281	17.638912	-0.105951	2.880560
563.065174	2764.014037	17.643917	-0.105952	2.876606
562.756685	2756.077737	17.648922	-0.105889	2.872650
562.355033	2748.142316	17.653927	-0.105809	2.868683
562.766740	2740.055477	17.658931	-0.105881	2.864682
562.732273	2732.122789	17.663936	-0.105869	2.860726
562.646245	2724.131293	17.668941	-0.105848	2.856733
563.093056	2716.074977	17.673946	-0.105926	2.852731
563.201615	2708.102435	17.678951	-0.105941	2.848747
563.298046	2700.106885	17.683955	-0.105953	2.844746
563.239276	2692.201765	17.688960	-0.105937	2.840775
563.174243	2684.259406	17.693965	-0.105920	2.836779
562.996566	2676.269874	17.698970	-0.105882	2.832748
563.183260	2668.264300	17.703975	-0.105911	2.828724
563.145101	2660.248847	17.708979	-0.105899	2.824676
562.787803	2652.365534	17.713984	-0.105827	2.820670
562.853021	2644.365453	17.718989	-0.105834	2.816624
562.784555	2636.371326	17.723994	-0.105816	2.812568
563.017320	2628.361338	17.728999	-0.105854	2.808515
562.933185	2620.382891	17.734003	-0.105833	2.804454
562.906494	2612.474340	17.739008	-0.105823	2.800426
562.712608	2604.534797	17.744013	-0.105782	2.796367
562.791088	2596.518387	17.749018	-0.105791	2.792278
562.586847	2588.573458	17.754023	-0.105748	2.788203
561.817857	2580.663522	17.759027	-0.105599	2.784106
561.683629	2572.700579	17.764032	-0.105569	2.780014
561.995170	2564.623743	17.769037	-0.105622	2.775885
561.825607	2556.636405	17.774042	-0.105585	2.771766
561.842304	2548.667009	17.779047	-0.105583	2.767661
562.190943	2540.589940	17.784051	-0.105642	2.763515
561.994807	2532.694667	17.789056	-0.105601	2.759424
561.871278	2524.758629	17.794061	-0.105572	2.755310
561.963009	2516.683849	17.799066	-0.105584	2.751131
561.627324	2508.763271	17.804071	-0.105517	2.746999
561.611740	2500.765207	17.809075	-0.105508	2.742840
561.959952	2492.765410	17.814080	-0.105568	2.738697
562.170137	2484.754460	17.819085	-0.105602	2.734533
562.116641	2476.794794	17.824090	-0.105587	2.730374
561.983650	2468.867516	17.829095	-0.105557	2.726219
562.125911	2460.861699	17.834099	-0.105578	2.722035
561.721208	2452.974670	17.839104	-0.105497	2.717872
561.425918	2445.039917	17.844109	-0.105437	2.713685
561.531944	2436.997612	17.849114	-0.105452	2.709459
561.270559	2429.076536	17.854119	-0.105398	2.705268
561.164169	2421.094234	17.859123	-0.105373	2.701048
561.197664	2413.115833	17.864128	-0.105374	2.696832
561.324291	2405.100916	17.869133	-0.105392	2.692596
560.774459	2397.195788	17.874138	-0.105284	2.688368
560.675165	2389.236991	17.879143	-0.105261	2.684134
560.754497	2381.231570	17.884147	-0.105270	2.679880
560.961367	2373.239677	17.889152	-0.105304	2.675635
561.045917	2365.225579	17.894157	-0.105314	2.671363
561.159792	2357.215998	17.899162	-0.105330	2.667088
560.728082	2349.320297	17.904167	-0.105244	2.662833
560.986847	2341.277259	17.909171	-0.105287	2.658536
561.397809	2333.268464	17.914176	-0.105359	2.654261
561.332354	2325.327110	17.919181	-0.105341	2.649984
560.708945	2317.455713	17.924186	-0.105220	2.645701
560.810974	2309.492387	17.929191	-0.105234	2.641409
560.865962	2301.466106	17.934195	-0.105239	2.637073
560.851786	2293.514826	17.939200	-0.105231	2.632766
560.699211	2285.554023	17.944205	-0.105197	2.628438
560.690916	2277.554362	17.949210	-0.105190	2.624091
560.745131	2269.599166	17.954215	-0.105195	2.619765
560.646761	2261.630857	17.959219	-0.105172	2.615414
560.722276	2253.637906	17.964224	-0.105180	2.611055
560.633363	2245.692184	17.969229	-0.105159	2.606703
560.568571	2237.726303	17.974234	-0.105141	2.602334
560.606869	2229.782809	17.979239	-0.105143	2.597977
560.465536	2221.798535	17.984243	-0.105112	2.593579
560.408841	2213.719824	17.989248	-0.105096	2.589126
559.760578	2205.853301	17.994253	-0.104970	2.584742
560.032530	2197.845053	17.999258	-0.105015	2.580336
560.288967	2189.838465	18.004263	-0.105058	2.575922
560.116871	2181.886096	18.009267	-0.105021	2.571501
560.264107	2173.896132	18.014272	-0.105043	2.567073
560.001126	2165.997089	18.019277	-0.104989	2.562660
559.885306	2158.029319	18.024282	-0.104962	2.558211
559.842049	2150.093066	18.029287	-0.104948	2.553777
559.675446	2142.113260	18.034291	-0.104912	2.549303
559.457905	2134.150996	18.039296	-0.104866	2.544826
559.469398	2126.201126	18.044301	-0.104863	2.540365
559.425649	2118.225949	18.049306	-0.104850	2.535878
559.595875	2110.239434	18.054311	-0.104876	2.531392
559.118777	2102.302481	18.059315	-0.104782	2.526879
559.319652	2094.316878	18.064320	-0.104815	2.522380
559.026571	2086.424663	18.069325	-0.104755	2.517889
558.753753	2078.461886	18.074330	-0.104699	2.513352
558.685940	2070.475662	18.079335	-0.104681	2.508809
558.726920	2062.454813	18.084339	-0.104683	2.504245
559.398031	2054.386110	18.089344	-0.104803	2.499693
558.847489	2046.534303	18.094349	-0.104695	2.495165
558.865803	2038.551833	18.099354	-0.104693	2.490597
558.820062	2030.592049	18.104359	-0.104680	2.486029
558.441913	2022.677998	18.109363	-0.104604	2.481453
558.400583	2014.730234	18.114368	-0.104591	2.476875
558.778982	2006.683672	18.119373	-0.104656	2.472263
558.432656	1998.764504	18.124378	-0.104587	2.467661
558.850489	1990.738649	18.129383	-0.104659	2.463047
558.677838	1982.825208	18.134387	-0.104622	2.458445
558.370648	1974.892294	18.139392	-0.104559	2.453812
558.490096	1966.892420	18.144397	-0.104576	2.449164
558.825201	1958.849814	18.149402	-0.104634	2.444499
558.657409	1950.985323	18.154407	-0.104597	2.439890
558.597903	1943.021054	18.159411	-0.104581	2.435223
558.445693	1935.060693	18.164416	-0.104547	2.430542
558.436497	1927.093615	18.169421	-0.104540	2.425859
558.370081	1919.127535	18.174426	-0.104523	2.421162
557.953341	1911.251272	18.179431	-0.104440	2.416483
557.768268	1903.278959	18.184435	-0.104400	2.411755
557.190901	1895.396546	18.189440	-0.104288	2.407041
556.937268	1887.431535	18.194445	-0.104235	2.402293
557.022433	1879.421386	18.199450	-0.104246	2.397537
557.084436	1871.456604	18.204455	-0.104252	2.392796
556.861764	1863.492973	18.209459	-0.104205	2.388023
556.806103	1855.522968	18.214464	-0.104190	2.383251
557.025363	1847.524175	18.219469	-0.104225	2.378474
557.158599	1839.522249	18.224474	-0.104245	2.373678
556.809702	1831.634073	18.229479	-0.104175	2.368902
556.908893	1823.643320	18.234483	-0.104188	2.364091
557.126148	1815.663625	18.239488	-0.104223	2.359287
557.260566	1807.713055	18.244493	-0.104243	2.354484
556.753027	1799.820460	18.249498	-0.104143	2.349653
556.605669	1791.881133	18.254503	-0.104111	2.344813
556.578615	1783.911718	18.259507	-0.104100	2.339955
556.862962	1775.910054	18.264512	-0.104148	2.335093
556.732298	1767.976628	18.269517	-0.104118	2.330228
556.616055	1760.024557	18.274522	-0.104092	2.325343
556.686126	1752.075451	18.279527	-0.104099	2.320465
556.786181	1744.092292	18.284531	-0.104113	2.315558
556.611500	1736.159877	18.289536	-0.104075	2.310649
556.577027	1728.214320	18.294541	-0.104063	2.305733
556.342622	1720.279505	18.299546	-0.104015	2.300796
556.263158	1712.373666	18.304551	-0.103995	2.295880
556.050040	1704.435090	18.309555	-0.103950	2.290921
555.571542	1696.538747	18.314560	-0.103855	2.285955
555.975756	1688.481874	18.319565	-0.103925	2.280954
555.836204	1680.557790	18.324570	-0.103894	2.275978
555.770567	1672.593672	18.329575	-0.103877	2.270973
555.831718	1664.587895	18.334579	-0.103883	2.265941
556.019876	1656.598000	18.339584	-0.103913	2.260919
555.762301	1648.711249	18.344589	-0.103859	2.255913
555.645572	1640.748670	18.349594	-0.103832	2.250859
555.614769	1632.817091	18.354599	-0.103822	2.245821
555.936238	1624.808452	18.359603	-0.103876	2.240754
555.606435	1616.928973	18.364608	-0.103810	2.235700
556.117960	1608.901203	18.369613	-0.103900	2.230615
555.609846	1601.038243	18.374618	-0.103800	2.225532
555.311605	1593.153140	18.379623	-0.103739	2.220443
555.403711	1585.165670	18.384627	-0.103751	2.215311
555.574466	1577.177799	18.389632	-0.103777	2.210174
555.065951	1569.324559	18.394637	-0.103678	2.205050
555.534288	1561.270920	18.399642	-0.103760	2.199874
555.669863	1553.349019	18.404647	-0.103780	2.194740
555.503138	1545.419205	18.409651	-0.103743	2.189562
555.677315	1537.426635	18.414656	-0.103770	2.184362
555.320112	1529.576185	18.419661	-0.103699	2.179193
554.991056	1521.677825	18.424666	-0.103632	2.173983
555.018859	1513.723781	18.429671	-0.103632	2.168757
554.566915	1505.830632	18.434675	-0.103543	2.163513
554.758869	1497.849056	18.439680	-0.103573	2.158259
554.721129	1489.878436	18.444685	-0.103561	2.152978
554.459667	1481.964623	18.449690	-0.103507	2.147700
554.674406	1473.985208	18.454695	-0.103542	2.142411
554.324156	1466.094148	18.459699	-0.103472	2.137113
553.961768	1458.212983	18.464704	-0.103399	2.131808
554.183734	1450.219790	18.469709	-0.103435	2.126471
554.103542	1442.267355	18.474714	-0.103415	2.121119
553.935657	1434.369224	18.479719	-0.103378	2.115781
553.979137	1426.352532	18.484723	-0.103381	2.110369
554.099583	1418.382027	18.489728	-0.103399	2.104983
554.151706	1410.455730	18.494733	-0.103403	2.099607
553.991727	1402.544534	18.499738	-0.103368	2.094206
553.970671	1394.612621	18.504743	-0.103359	2.088790
553.813197	1386.689248	18.509747	-0.103324	2.083353
553.597894	1378.806000	18.514752	-0.103279	2.077923
553.773251	1370.850633	18.519757	-0.103307	2.072469
553.858423	1362.868209	18.524762	-0.103317	2.066972
553.956506	1354.924878	18.529767	-0.103330	2.061489
553.227503	1347.132176	18.534771	-0.103189	2.056012
553.658648	1339.105456	18.539776	-0.103264	2.050476
553.432933	1331.217868	18.544781	-0.103217	2.044955
552.843635	1323.391206	18.549786	-0.103102	2.039423
553.327805	1315.364596	18.554791	-0.103187	2.033848
553.720977	1307.333761	18.559795	-0.103255	2.028244
554.015356	1299.355086	18.564800	-0.103305	2.022652
553.846886	1291.504430	18.569805	-0.103268	2.017086
553.754705	1283.594294	18.574810	-0.103246	2.011471
553.482202	1275.720981	18.579815	-0.103190	2.005847
553.215061	1267.842896	18.584819	-0.103135	2.000205
553.185816	1259.915417	18.589824	-0.103124	1.994536
553.399488	1251.956239	18.594829	-0.103159	1.988855
553.170002	1244.038198	18.599834	-0.103111	1.983139
553.478032	1236.081693	18.604839	-0.103163	1.977437
553.021313	1228.250124	18.609843	-0.103073	1.971726
552.732346	1220.350258	18.614848	-0.103014	1.965967
552.649226	1212.455968	18.619853	-0.102993	1.960217
552.469818	1204.557013	18.624858	-0.102955	1.954437
552.192234	1196.668382	18.629863	-0.102898	1.948636
552.084336	1188.712687	18.634867	-0.102872	1.942787
552.233110	1180.732380	18.639872	-0.102895	1.936931
552.349243	1172.781608	18.644877	-0.102911	1.931075
552.453273	1164.830334	18.649882	-0.102925	1.925200
552.609542	1156.924275	18.654887	-0.102949	1.919347
552.610751	1149.008738	18.659891	-0.102944	1.913451
552.698061	1141.074053	18.664896	-0.102955	1.907532
552.813184	1133.157169	18.669901	-0.102972	1.901611
552.392870	1125.344127	18.674906	-0.102888	1.895689
551.853116	1117.523789	18.679911	-0.102783	1.889729
552.152774	1109.533895	18.684915	-0.102833	1.883718
551.987634	1101.659838	18.689920	-0.102797	1.877722
552.172873	1093.710434	18.694925	-0.102826	1.871690
551.559631	1085.883300	18.699930	-0.102707	1.865639
551.402463	1077.992282	18.704935	-0.102673	1.859573
551.565653	1070.039884	18.709939	-0.102698	1.853477
551.650354	1062.087335	18.714944	-0.102708	1.847352
551.213914	1054.270759	18.719949	-0.102622	1.841250
550.909249	1046.409795	18.724954	-0.102560	1.835108
551.018411	1038.474403	18.729959	-0.102575	1.828938
550.740901	1030.594624	18.734963	-0.102518	1.822743
551.099488	1022.624495	18.739968	-0.102580	1.816534
551.243509	1014.715034	18.744973	-0.102601	1.810325
550.683745	1006.893208	18.749978	-0.102492	1.804077
551.234670	998.910978	18.754983	-0.102589	1.797818
551.378453	990.979445	18.759987	-0.102611	1.791526
551.342555	983.066633	18.764992	-0.102599	1.785205
551.006844	975.273432	18.769997	-0.102532	1.778920
550.874975	967.384787	18.775002	-0.102502	1.772562
550.738255	959.505003	18.780007	-0.102471	1.766187
550.652309	951.639467	18.785011	-0.102450	1.759807
550.680121	943.742899	18.790016	-0.102450	1.753392
550.342598	935.928542	18.795021	-0.102382	1.746975
550.339456	927.998249	18.800026	-0.102376	1.740482
550.058637	920.180528	18.805031	-0.102319	1.734021
550.827763	912.132689	18.810035	-0.102457	1.727483
550.344958	904.358950	18.815040	-0.102362	1.720983
550.720901	896.415391	18.820045	-0.102426	1.714430
550.120932	888.643030	18.825050	-0.102310	1.707867
550.076324	880.763702	18.830055	-0.102296	1.701262
549.823915	872.927996	18.835059	-0.102244	1.694640
549.194800	865.144547	18.840064	-0.102122	1.687985
549.570712	857.179925	18.845069	-0.102187	1.681286
549.258557	849.348117	18.850074	-0.102123	1.674580
548.941801	841.528425	18.855079	-0.102059	1.667857
548.973156	833.622487	18.860083	-0.102060	1.661080
549.350480	825.673534	18.865088	-0.102125	1.654285
548.770993	817.917651	18.870093	-0.102012	1.647498
548.985180	809.991129	18.875098	-0.102046	1.640644
548.825051	802.167632	18.880103	-0.102012	1.633800
548.869286	794.249505	18.885107	-0.102015	1.626872
549.135160	786.316192	18.890112	-0.102059	1.619932
548.922071	778.533741	18.895117	-0.102014	1.613028
549.095801	770.623950	18.900122	-0.102041	1.606037
549.022459	762.810275	18.905127	-0.102022	1.599065
549.281782	754.922293	18.910131	-0.102066	1.592044
549.061006	747.105756	18.915136	-0.102019	1.584987
548.804004	739.354713	18.920141	-0.101966	1.577952
548.170101	731.591992	18.925146	-0.101843	1.570819
547.988532	723.771302	18.930151	-0.101804	1.563668
548.589412	715.798196	18.935155	-0.101911	1.556460
548.102505	708.058800	18.940160	-0.101815	1.549272
547.911226	700.242895	18.945165	-0.101774	1.542023
548.236394	692.329940	18.950170	-0.101830	1.534728
548.326873	684.478135	18.955175	-0.101841	1.527420
548.321219	676.651785	18.960179	-0.101835	1.520086
547.968252	668.908518	18.965184	-0.101764	1.512741
547.564883	661.149029	18.970189	-0.101684	1.505337
547.643714	653.301622	18.975194	-0.101694	1.497887
547.275082	645.542825	18.980199	-0.101620	1.490416
547.329765	637.693613	18.985203	-0.101625	1.482886
547.632894	629.819639	18.990208	-0.101676	1.475333
547.548308	621.999921	18.995213	-0.101655	1.467732
547.309267	614.222157	19.000218	-0.101606	1.460108
547.451790	606.396041	19.005223	-0.101627	1.452457
547.195853	598.625197	19.010227	-0.101574	1.444757
546.923612	590.886743	19.015232	-0.101519	1.437044
547.082956	583.045340	19.020237	-0.101543	1.429258
547.196214	575.212162	19.025242	-0.101559	1.421430
547.524009	567.387128	19.030247	-0.101615	1.413602
547.395992	559.625413	19.035251	-0.101586	1.405719
547.053187	551.927788	19.040256	-0.101517	1.397820
546.932979	544.180801	19.045261	-0.101490	1.389864
546.701174	536.416391	19.050266	-0.101441	1.381824
546.477015	528.698176	19.055271	-0.101395	1.373787
546.281222	520.944272	19.060275	-0.101353	1.365670
546.495060	513.132479	19.065280	-0.101388	1.357515
546.184731	505.437488	19.070285	-0.101325	1.349343
546.338778	497.612486	19.075290	-0.101348	1.341064
546.322566	489.883757	19.080295	-0.101340	1.332807
546.058796	482.179998	19.085299	-0.101286	1.324480
545.974732	474.450794	19.090304	-0.101265	1.316105
546.521293	466.517780	19.095309	-0.101362	1.307571
546.508101	458.779430	19.100314	-0.101354	1.299090
546.338888	451.096142	19.105319	-0.101318	1.290586
546.200538	443.412472	19.110323	-0.101287	1.282031
545.981102	435.752041	19.115328	-0.101241	1.273429
545.621262	428.101080	19.120333	-0.101169	1.264752
546.095679	420.301285	19.125338	-0.101252	1.256006
545.429882	412.728630	19.130343	-0.101123	1.247238
545.712142	404.978855	19.135347	-0.101171	1.238389
545.502419	397.312730	19.140352	-0.101127	1.229477
545.262278	389.669661	19.145357	-0.101077	1.220520
545.631357	381.905709	19.150362	-0.101141	1.211476
545.726220	374.223436	19.155367	-0.101153	1.202406
545.587384	366.603675	19.160371	-0.101122	1.193295
545.413132	358.968030	19.165376	-0.101085	1.184087
545.691587	351.272398	19.170381	-0.101132	1.174827
545.401075	343.679330	19.175386	-0.101073	1.165501
545.064429	336.123085	19.180391	-0.101005	1.156135
545.164241	328.434101	19.185395	-0.101019	1.146620
545.280808	320.778518	19.190400	-0.101035	1.137071
544.866845	313.246545	19.195405	-0.100953	1.127483
544.982347	305.625542	19.200410	-0.100970	1.117814
544.556978	298.103746	19.205415	-0.100886	1.108069
544.874387	290.446410	19.210419	-0.100940	1.098228
544.951486	282.854510	19.215424	-0.100949	1.088329
545.096237	275.275089	19.220429	-0.100971	1.078371
545.150673	267.706098	19.225434	-0.100976	1.068314
544.790845	260.231126	19.230439	-0.100904	1.058191
544.802709	252.684350	19.235443	-0.100901	1.047961
544.419891	245.236193	19.240448	-0.100825	1.037671
543.855537	237.827467	19.245453	-0.100715	1.027288
543.893784	230.302892	19.250458	-0.100718	1.016784
543.805593	222.809317	19.255463	-0.100696	1.006183
543.623745	215.367912	19.260467	-0.100657	0.995520
543.684150	207.844871	19.265472	-0.100664	0.984684
543.698369	200.388671	19.270477	-0.100661	0.973815
543.250381	193.011828	19.275482	-0.100573	0.962820
543.799579	185.493210	19.280487	-0.100671	0.951747
543.562007	178.134084	19.285491	-0.100621	0.940577
543.230818	170.800394	19.290496	-0.100555	0.929287
543.355997	163.408647	19.295501	-0.100573	0.917891
542.974364	156.115850	19.300506	-0.100498	0.906369
542.731256	148.811338	19.305511	-0.100447	0.894717
542.874510	141.450300	19.310515	-0.100469	0.882931
542.407835	134.247794	19.315520	-0.100378	0.871069
542.385960	126.969257	19.320525	-0.100369	0.859046
542.424016	119.693796	19.325530	-0.100371	0.846876
542.183911	112.504514	19.330535	-0.100322	0.834592
542.238300	105.263155	19.335539	-0.100327	0.822124
542.098347	98.097365	19.340544	-0.100296	0.809537
542.451997	90.879113	19.345549	-0.100357	0.796814
541.973070	83.838873	19.350554	-0.100264	0.783940
541.904089	76.755533	19.355559	-0.100246	0.770905
542.338975	69.800620	19.360563	-0.100322	0.758057