Mon Apr 19 09:00:04 2021

Number of Points = 3641
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.049753	-0.060390	0.000000	0.000011	0.307709

2.028264	-0.058437	0.005005	0.000015	0.307700
1.775875	-0.011074	0.010010	0.000062	0.307707
1.974430	-0.046053	0.015014	0.000025	0.307711
1.692764	0.005040	0.020019	0.000078	0.307711
1.894552	-0.030841	0.025024	0.000040	0.307714
2.245859	-0.098338	0.030029	-0.000025	0.307697
1.994517	-0.050879	0.035034	0.000022	0.307705
2.186697	-0.084803	0.040038	-0.000014	0.307710
1.915538	-0.036237	0.045043	0.000036	0.307706
2.402575	-0.124960	0.050048	-0.000054	0.307705
1.791591	-0.010931	0.055053	0.000060	0.307719
1.299757	0.080847	0.060058	0.000151	0.307730
1.744893	-0.001146	0.065062	0.000068	0.307724
1.828145	-0.019851	0.070067	0.000053	0.307707
1.673078	-0.006971	0.075072	0.000082	0.307635
1.499265	-0.023714	0.080077	0.000114	0.307408
1.893496	-0.099583	0.085082	0.000041	0.307388
1.649536	-0.050693	0.090086	0.000086	0.307409
1.925526	-0.103818	0.095091	0.000035	0.307395
1.966218	-0.109136	0.100096	0.000027	0.307404
2.035985	-0.124119	0.105101	0.000015	0.307393
2.097555	-0.140298	0.110106	0.000003	0.307369
2.529789	-0.286164	0.115110	-0.000077	0.307052
2.440318	-0.271933	0.120115	-0.000061	0.307042
2.206318	-0.226129	0.125120	-0.000017	0.307058
2.348030	-0.253673	0.130125	-0.000043	0.307049
1.992253	-0.216713	0.135130	0.000023	0.306918
2.109361	-0.269347	0.140134	0.000001	0.306770
2.402901	-0.325614	0.145139	-0.000053	0.306756
1.901889	-0.227725	0.150144	0.000040	0.306788
2.209559	-0.314616	0.155149	-0.000017	0.306642
2.234734	-0.364486	0.160154	-0.000022	0.306428
2.471026	-0.406199	0.165158	-0.000066	0.306433
2.416343	-0.398525	0.170163	-0.000056	0.306423
2.669495	-0.502410	0.175168	-0.000103	0.306149
2.431715	-0.465539	0.180173	-0.000058	0.306119
2.274176	-0.434966	0.185178	-0.000029	0.306128
2.267155	-0.485391	0.190182	-0.000027	0.305883
2.514582	-0.549745	0.195187	-0.000073	0.305791
2.467498	-0.538679	0.200192	-0.000065	0.305803
2.194397	-0.535760	0.205197	-0.000014	0.305582
2.505686	-0.603191	0.210202	-0.000072	0.305530
2.622464	-0.630785	0.215206	-0.000093	0.305499
2.235481	-0.623069	0.220211	-0.000021	0.305203
2.444046	-0.661997	0.225216	-0.000060	0.305197
2.369685	-0.683491	0.230221	-0.000046	0.305031
2.118404	-0.668223	0.235226	0.000001	0.304887
2.066190	-0.656664	0.240230	0.000010	0.304896
1.732654	-0.664589	0.245235	0.000073	0.304571
2.251269	-0.761564	0.250240	-0.000024	0.304558
2.385931	-0.820034	0.255245	-0.000049	0.304396
2.296072	-0.831479	0.260250	-0.000032	0.304264
2.499707	-0.886309	0.265254	-0.000070	0.304179
2.816741	-1.000730	0.270259	-0.000129	0.303908
2.168920	-0.889536	0.275264	-0.000008	0.303877
2.328741	-0.972982	0.280269	-0.000038	0.303617
2.043794	-0.920380	0.285274	0.000015	0.303621
2.256487	-1.023647	0.290278	-0.000024	0.303313
1.926101	-0.965643	0.295283	0.000037	0.303303
1.987715	-1.031635	0.300288	0.000026	0.303041
2.016823	-1.039516	0.305293	0.000021	0.303029
1.531485	-1.016545	0.310298	0.000111	0.302717
1.892544	-1.089604	0.315302	0.000044	0.302681
1.459494	-1.067340	0.320307	0.000124	0.302411
1.316742	-1.045506	0.325312	0.000151	0.302391
1.651401	-1.165657	0.330317	0.000089	0.302107
2.024743	-1.248641	0.335322	0.000019	0.302034
2.209197	-1.335937	0.340326	-0.000015	0.301776
1.726851	-1.260401	0.345331	0.000075	0.301718
1.794839	-1.332105	0.350336	0.000062	0.301433
1.960645	-1.385351	0.355341	0.000032	0.301322
1.993788	-1.434486	0.360346	0.000026	0.301114
2.441113	-1.558370	0.365350	-0.000058	0.300909
2.012685	-1.503991	0.370355	0.000022	0.300796
2.108060	-1.570956	0.375360	0.000005	0.300557
1.329751	-1.448547	0.380365	0.000149	0.300465
1.352476	-1.502205	0.385370	0.000145	0.300227
1.392982	-1.547799	0.390374	0.000138	0.300042
1.592955	-1.613441	0.395379	0.000101	0.299901
1.415150	-1.642215	0.400384	0.000134	0.299605
1.081779	-1.601856	0.405389	0.000196	0.299508
1.253937	-1.675152	0.410394	0.000164	0.299304
1.690488	-1.804593	0.415398	0.000083	0.299062
1.776237	-1.855666	0.420403	0.000067	0.298890
2.171522	-1.980422	0.425408	-0.000007	0.298633
2.147539	-2.029193	0.430413	-0.000002	0.298376
1.855403	-2.010851	0.435418	0.000052	0.298207
1.991494	-2.073444	0.440422	0.000027	0.298023
0.896036	-1.932794	0.445427	0.000231	0.297739
1.360891	-2.049978	0.450432	0.000145	0.297580
1.691163	-2.151730	0.455437	0.000083	0.297376
1.202242	-2.124892	0.460442	0.000174	0.297074
1.243185	-2.166385	0.465446	0.000167	0.296908
1.590349	-2.273922	0.470451	0.000102	0.296691
1.152950	-2.242513	0.475456	0.000184	0.296456
1.081362	-2.281315	0.480461	0.000197	0.296203
0.705186	-2.251002	0.485466	0.000267	0.296017
0.780307	-2.300580	0.490470	0.000253	0.295841
0.452086	-2.290576	0.495475	0.000314	0.295598
0.660381	-2.370634	0.500480	0.000276	0.295391
0.743099	-2.429335	0.505485	0.000260	0.295177
0.597137	-2.452115	0.510490	0.000288	0.294935
0.378204	-2.470655	0.515494	0.000328	0.294648
0.327362	-2.499367	0.520499	0.000338	0.294462
0.541226	-2.577931	0.525504	0.000298	0.294266
0.579517	-2.641954	0.530509	0.000291	0.293985
0.223898	-2.631623	0.535514	0.000357	0.293718
-0.844621	-2.477953	0.540518	0.000556	0.293518
-1.686944	-2.357921	0.545523	0.000713	0.293354
-1.805137	-2.391712	0.550528	0.000735	0.293081
-1.946637	-2.399945	0.555533	0.000762	0.292914
-2.253370	-2.382170	0.560538	0.000819	0.292726
-1.778582	-2.526756	0.565542	0.000731	0.292437
-2.381045	-2.450035	0.570547	0.000843	0.292275
-2.977212	-2.379375	0.575552	0.000954	0.292088
-3.148385	-2.392330	0.580557	0.000986	0.291869
-3.466663	-2.356545	0.585562	0.001045	0.291759
-3.706654	-2.369185	0.590566	0.001090	0.291480
-3.658911	-2.407360	0.595571	0.001081	0.291333
-3.640161	-2.446060	0.600576	0.001077	0.291158
-3.920346	-2.447471	0.605581	0.001130	0.290897
-3.935775	-2.468411	0.610586	0.001133	0.290779
-4.079621	-2.484183	0.615590	0.001159	0.290570
-4.437458	-2.452028	0.620595	0.001226	0.290406
-4.774968	-2.426549	0.625600	0.001289	0.290227
-4.554745	-2.516126	0.630605	0.001248	0.289979
-4.606489	-2.532163	0.635610	0.001258	0.289852
-5.176796	-2.484711	0.640614	0.001364	0.289571
-4.932038	-2.553871	0.645619	0.001318	0.289448
-4.808992	-2.613189	0.650624	0.001296	0.289263
-5.640824	-2.507526	0.655629	0.001450	0.289034
-5.913409	-2.478140	0.660634	0.001501	0.288933
-5.889568	-2.536037	0.665638	0.001497	0.288665
-5.970458	-2.540843	0.670643	0.001512	0.288567
-6.415757	-2.512639	0.675648	0.001595	0.288302
-6.324428	-2.550527	0.680653	0.001578	0.288195
-6.864932	-2.488570	0.685658	0.001679	0.288012
-6.857303	-2.525588	0.690662	0.001677	0.287833
-7.005594	-2.532284	0.695667	0.001705	0.287663
-6.976798	-2.582087	0.700672	0.001700	0.287439
-7.174638	-2.564161	0.705677	0.001737	0.287348
-7.685860	-2.530089	0.710682	0.001832	0.287051
-7.084079	-2.649200	0.715686	0.001720	0.287002
-7.648742	-2.601205	0.720691	0.001825	0.286726
-7.769870	-2.597329	0.725696	0.001848	0.286634
-8.517107	-2.505162	0.730701	0.001987	0.286413
-8.382803	-2.551352	0.735706	0.001962	0.286303
-8.764615	-2.521884	0.740710	0.002033	0.286100
-8.989949	-2.504282	0.745715	0.002075	0.285982
-9.432224	-2.458767	0.750720	0.002157	0.285805
-9.549664	-2.451400	0.755725	0.002179	0.285734
-10.044044	-2.397570	0.760730	0.002271	0.285551
-9.136115	-2.578663	0.765734	0.002102	0.285470
-10.208295	-2.438207	0.770739	0.002302	0.285193
-10.199832	-2.442131	0.775744	0.002300	0.285181
-10.249680	-2.490992	0.780749	0.002310	0.284886
-10.713228	-2.406110	0.785754	0.002396	0.284889
-10.455474	-2.513092	0.790758	0.002348	0.284583
-11.155275	-2.388310	0.795763	0.002478	0.284571
-10.977670	-2.461093	0.800768	0.002445	0.284365
-10.903219	-2.495065	0.805773	0.002432	0.284260
-11.373993	-2.445527	0.810778	0.002519	0.284076
-11.126259	-2.519118	0.815782	0.002473	0.283931
-11.259261	-2.520976	0.820787	0.002498	0.283798
-11.778396	-2.462051	0.825792	0.002595	0.283617
-11.815620	-2.465034	0.830797	0.002602	0.283567
-12.098732	-2.466860	0.835802	0.002655	0.283294
-12.172103	-2.448931	0.840806	0.002668	0.283317
-12.793126	-2.391457	0.845811	0.002784	0.283034
-12.863389	-2.380321	0.850816	0.002797	0.283025
-12.929723	-2.404660	0.855821	0.002809	0.282839
-13.793062	-2.277320	0.860826	0.002970	0.282687
-12.911340	-2.442940	0.865830	0.002806	0.282659
-13.258167	-2.437085	0.870835	0.002871	0.282366
-13.501016	-2.393133	0.875840	0.002916	0.282365
-13.984686	-2.345177	0.880845	0.003006	0.282160
-14.241659	-2.318972	0.885850	0.003054	0.282054
-14.184588	-2.336962	0.890854	0.003043	0.282015
-14.735973	-2.285679	0.895859	0.003146	0.281763
-14.021669	-2.416557	0.900864	0.003013	0.281758
-14.018308	-2.457822	0.905869	0.003013	0.281549
-14.745105	-2.352022	0.910874	0.003148	0.281413
-14.595698	-2.384868	0.915878	0.003120	0.281383
-15.137172	-2.334043	0.920883	0.003221	0.281138
-15.099090	-2.342261	0.925888	0.003214	0.281131
-15.227298	-2.357240	0.930893	0.003238	0.280934
-15.537714	-2.325526	0.935898	0.003296	0.280806
-15.211865	-2.387335	0.940902	0.003235	0.280793
-15.577575	-2.366287	0.945907	0.003303	0.280558
-15.607128	-2.356565	0.950912	0.003309	0.280580
-15.340824	-2.447594	0.955917	0.003259	0.280360
-16.221251	-2.314695	0.960922	0.003423	0.280219
-15.947946	-2.366102	0.965926	0.003372	0.280210
-16.216201	-2.374286	0.970931	0.003422	0.279916
-16.789400	-2.267699	0.975936	0.003529	0.279928
-16.685119	-2.315777	0.980941	0.003510	0.279777
-16.979730	-2.295780	0.985946	0.003565	0.279603
-16.649504	-2.356216	0.990950	0.003503	0.279601
-17.195811	-2.307404	0.995955	0.003605	0.279339
-16.963555	-2.358109	1.000960	0.003562	0.279295
-16.953654	-2.374312	1.005965	0.003560	0.279220
-17.578796	-2.311249	1.010970	0.003676	0.278957
-17.015404	-2.413279	1.015974	0.003572	0.278959
-17.264990	-2.411015	1.020979	0.003618	0.278735
-17.770238	-2.335837	1.025984	0.003712	0.278648
-17.521302	-2.397320	1.030989	0.003666	0.278563
-18.032784	-2.350606	1.035994	0.003761	0.278322
-17.454198	-2.455914	1.040998	0.003654	0.278322
-18.206148	-2.362545	1.046003	0.003794	0.278096
-18.016363	-2.412375	1.051008	0.003758	0.278016
-18.127360	-2.404276	1.056013	0.003779	0.277953
-19.037694	-2.287961	1.061018	0.003949	0.277696
-18.695685	-2.350394	1.066022	0.003885	0.277695
-18.287261	-2.465862	1.071027	0.003809	0.277479
-19.303804	-2.298549	1.076032	0.003998	0.277388
-18.836264	-2.391431	1.081037	0.003911	0.277346
-19.122780	-2.395712	1.086042	0.003965	0.277052
-18.812266	-2.451035	1.091046	0.003907	0.277057
-19.482903	-2.365089	1.096051	0.004032	0.276869
-19.414662	-2.400830	1.101056	0.004019	0.276747
-19.024899	-2.478392	1.106061	0.003947	0.276712
-19.968584	-2.359940	1.111066	0.004122	0.276433
-19.587586	-2.431512	1.116070	0.004051	0.276421
-19.610935	-2.465290	1.121075	0.004056	0.276221
-20.408222	-2.337855	1.126080	0.004204	0.276129
-20.596075	-2.304755	1.131085	0.004239	0.276123
-20.519874	-2.380387	1.136090	0.004225	0.275799
-20.540355	-2.372462	1.141094	0.004229	0.275821
-20.421747	-2.419677	1.146099	0.004207	0.275686
-20.903353	-2.355147	1.151104	0.004297	0.275565
-20.450624	-2.437975	1.156109	0.004213	0.275562
-20.927944	-2.415641	1.161114	0.004301	0.275223
-20.809199	-2.438233	1.166118	0.004279	0.275217
-21.244805	-2.385892	1.171123	0.004361	0.275076
-21.697524	-2.333652	1.176128	0.004445	0.274917
-21.422819	-2.384761	1.181133	0.004394	0.274911
-21.913235	-2.351847	1.186138	0.004485	0.274614
-21.142009	-2.499358	1.191142	0.004342	0.274576
-21.467350	-2.466543	1.196147	0.004402	0.274436
-22.053838	-2.389789	1.201152	0.004511	0.274278
-22.147744	-2.369625	1.206157	0.004529	0.274294
-22.374026	-2.389920	1.211162	0.004571	0.273970
-22.321504	-2.402998	1.216166	0.004561	0.273951
-22.259413	-2.438923	1.221171	0.004550	0.273820
-22.736310	-2.385493	1.226176	0.004639	0.273644
-22.782788	-2.377469	1.231181	0.004647	0.273641
-23.085527	-2.374026	1.236186	0.004704	0.273368
-23.181325	-2.363714	1.241190	0.004722	0.273330
-22.796429	-2.454287	1.246195	0.004650	0.273221
-23.231528	-2.413642	1.251200	0.004731	0.273017
-23.242993	-2.410766	1.256205	0.004733	0.273021
-23.593739	-2.396676	1.261210	0.004799	0.272757
-23.999288	-2.333176	1.266214	0.004874	0.272702
-23.688415	-2.401642	1.271219	0.004816	0.272638
-24.271297	-2.342936	1.276224	0.004925	0.272387
-24.539584	-2.293090	1.281229	0.004975	0.272392
-24.586792	-2.310166	1.286234	0.004984	0.272256
-23.908530	-2.472868	1.291238	0.004858	0.272046
-24.422842	-2.379342	1.296243	0.004953	0.272046
-24.344688	-2.442291	1.301248	0.004939	0.271786
-24.229930	-2.470868	1.306253	0.004918	0.271745
-24.683249	-2.412153	1.311258	0.005002	0.271618
-25.139900	-2.363100	1.316262	0.005087	0.271436
-25.340643	-2.326002	1.321267	0.005124	0.271439
-24.747617	-2.483210	1.326272	0.005014	0.271176
-25.293180	-2.392392	1.331277	0.005116	0.271131
-25.704174	-2.333889	1.336282	0.005192	0.271044
-26.203524	-2.280446	1.341286	0.005285	0.270844
-26.219019	-2.280628	1.346291	0.005288	0.270827
-26.095194	-2.328825	1.351296	0.005265	0.270690
-26.166174	-2.339246	1.356301	0.005279	0.270565
-26.403616	-2.296112	1.361306	0.005323	0.270564
-26.156949	-2.392328	1.366310	0.005277	0.270289
-26.549859	-2.337732	1.371315	0.005350	0.270199
-26.469150	-2.359663	1.376320	0.005335	0.270159
-26.698166	-2.367809	1.381325	0.005378	0.269892
-26.472273	-2.411989	1.386330	0.005336	0.269875
-26.399344	-2.460250	1.391334	0.005322	0.269687
-27.239111	-2.329474	1.396339	0.005479	0.269569
-26.723649	-2.433150	1.401344	0.005383	0.269516
-26.872809	-2.451712	1.406349	0.005411	0.269270
-27.384545	-2.356797	1.411354	0.005506	0.269279
-27.265729	-2.414816	1.416358	0.005484	0.269083
-28.056733	-2.295496	1.421363	0.005631	0.268951
-27.728463	-2.354713	1.426368	0.005570	0.268953
-27.901761	-2.378217	1.431373	0.005602	0.268657
-28.090662	-2.350523	1.436378	0.005638	0.268621
-27.930919	-2.398614	1.441382	0.005608	0.268518
-27.964192	-2.432046	1.446387	0.005614	0.268304
-28.823428	-2.271998	1.451392	0.005774	0.268325
-28.181582	-2.430743	1.456397	0.005655	0.268098
-28.022529	-2.478184	1.461402	0.005625	0.267997
-28.068760	-2.491919	1.466406	0.005634	0.267877
-28.753036	-2.405284	1.471411	0.005761	0.267673
-28.450820	-2.460931	1.476416	0.005705	0.267669
-28.711268	-2.466999	1.481421	0.005754	0.267379
-28.950324	-2.430456	1.486426	0.005798	0.267341
-28.053906	-2.627606	1.491430	0.005631	0.267156
-28.389112	-2.594394	1.496435	0.005694	0.267006
-29.037514	-2.494884	1.501440	0.005815	0.266905
-29.622775	-2.417291	1.506445	0.005924	0.266749
-29.276233	-2.483605	1.511450	0.005859	0.266731
-29.089762	-2.574434	1.516454	0.005825	0.266421
-29.892372	-2.432783	1.521459	0.005974	0.266397
-29.902330	-2.461614	1.526464	0.005976	0.266231
-29.538973	-2.555057	1.531469	0.005908	0.266081
-30.106710	-2.461277	1.536474	0.006014	0.266030
-30.137164	-2.502768	1.541478	0.006020	0.265773
-30.083725	-2.514146	1.546483	0.006010	0.265764
-30.435845	-2.489229	1.551488	0.006075	0.265550
-30.813103	-2.425074	1.556493	0.006146	0.265526
-30.830734	-2.445679	1.561498	0.006149	0.265396
-31.020396	-2.449261	1.566502	0.006184	0.265188
-30.864085	-2.480712	1.571507	0.006155	0.265171
-31.051804	-2.496916	1.576512	0.006190	0.264896
-31.422826	-2.432809	1.581517	0.006259	0.264877
-31.702176	-2.411124	1.586522	0.006311	0.264717
-31.825496	-2.420743	1.591526	0.006334	0.264542
-31.919844	-2.401484	1.596531	0.006352	0.264553
-31.862978	-2.458246	1.601536	0.006342	0.264298
-32.063419	-2.430907	1.606541	0.006379	0.264248
-32.079942	-2.451725	1.611546	0.006382	0.264117
-31.880570	-2.527169	1.616550	0.006345	0.263902
-32.545744	-2.404096	1.621555	0.006469	0.263913
-32.518013	-2.461971	1.626560	0.006464	0.263623
-32.543515	-2.460328	1.631565	0.006469	0.263606
-32.657633	-2.470041	1.636570	0.006490	0.263439
-33.232937	-2.392676	1.641574	0.006597	0.263288
-32.666948	-2.499389	1.646579	0.006492	0.263268
-32.976100	-2.494092	1.651584	0.006549	0.262987
-32.772663	-2.533390	1.656589	0.006512	0.262974
-32.748483	-2.577736	1.661594	0.006507	0.262754
-33.112201	-2.532692	1.666598	0.006575	0.262637
-33.505754	-2.477887	1.671603	0.006648	0.262544
-34.074507	-2.412139	1.676608	0.006754	0.262336
-33.327684	-2.548545	1.681613	0.006615	0.262333
-34.345414	-2.412699	1.686618	0.006805	0.262060
-34.627603	-2.367719	1.691622	0.006857	0.262025
-33.871443	-2.522170	1.696627	0.006716	0.261931
-34.043555	-2.530652	1.701632	0.006749	0.261711
-34.412698	-2.460818	1.706637	0.006817	0.261725
-35.236898	-2.361152	1.711642	0.006971	0.261447
-34.844771	-2.440804	1.716646	0.006898	0.261401
-35.025707	-2.422716	1.721651	0.006932	0.261318
-35.615014	-2.356439	1.726656	0.007041	0.261091
-35.350258	-2.402004	1.731661	0.006992	0.261105
-35.870351	-2.342815	1.736666	0.007089	0.260908
-35.496208	-2.437519	1.741670	0.007019	0.260760
-35.199948	-2.495955	1.746675	0.006964	0.260735
-35.630903	-2.454886	1.751680	0.007045	0.260527
-35.713628	-2.440782	1.756685	0.007060	0.260522
-35.562989	-2.509466	1.761690	0.007032	0.260292
-35.655338	-2.512899	1.766694	0.007049	0.260179
-35.845992	-2.493575	1.771699	0.007085	0.260093
-36.586919	-2.400065	1.776704	0.007223	0.259863
-35.886904	-2.527698	1.781709	0.007093	0.259861
-36.072025	-2.545353	1.786714	0.007127	0.259575
-36.614021	-2.455729	1.791718	0.007228	0.259524
-37.027089	-2.396025	1.796723	0.007305	0.259438
-37.212322	-2.394680	1.801728	0.007339	0.259257
-36.798987	-2.470461	1.806733	0.007263	0.259253
-37.102377	-2.468514	1.811738	0.007319	0.258956
-37.515011	-2.398006	1.816742	0.007396	0.258930
-37.665917	-2.387435	1.821747	0.007424	0.258835
-37.809450	-2.402611	1.826752	0.007451	0.258604
-37.426747	-2.470993	1.831757	0.007380	0.258610
-37.971266	-2.418532	1.836762	0.007481	0.258349
-37.939802	-2.437228	1.841766	0.007475	0.258276
-37.701724	-2.495329	1.846771	0.007431	0.258193
-37.901544	-2.497159	1.851776	0.007468	0.257978
-38.228497	-2.435057	1.856781	0.007529	0.257993
-38.436350	-2.452975	1.861786	0.007568	0.257680
-38.250268	-2.490701	1.866790	0.007533	0.257657
-38.380859	-2.494848	1.871795	0.007558	0.257500
-38.859326	-2.438387	1.876800	0.007647	0.257328
-38.956499	-2.416660	1.881805	0.007665	0.257351
-39.665854	-2.340922	1.886810	0.007797	0.257050
-39.397594	-2.392052	1.891814	0.007747	0.257037
-39.542000	-2.382250	1.896819	0.007774	0.256944
-39.933280	-2.344241	1.901824	0.007847	0.256756
-39.853449	-2.358648	1.906829	0.007832	0.256757
-40.420082	-2.292312	1.911834	0.007938	0.256549
-40.232794	-2.349034	1.916838	0.007903	0.256421
-40.194114	-2.357761	1.921843	0.007896	0.256411
-40.470131	-2.358039	1.926848	0.007947	0.256125
-40.243430	-2.402981	1.931853	0.007905	0.256104
-40.879594	-2.302769	1.936858	0.008023	0.256016
-41.177235	-2.285416	1.941862	0.008079	0.255808
-41.157481	-2.291002	1.946867	0.008075	0.255796
-40.988200	-2.345222	1.951872	0.008044	0.255663
-40.991710	-2.365671	1.956877	0.008044	0.255543
-41.428666	-2.286857	1.961882	0.008126	0.255539
-41.527191	-2.316709	1.966886	0.008144	0.255268
-41.435303	-2.343977	1.971891	0.008127	0.255208
-41.873549	-2.274431	1.976896	0.008209	0.255150
-42.253224	-2.247438	1.981901	0.008280	0.254911
-41.876178	-2.320020	1.986906	0.008209	0.254888
-42.188757	-2.286248	1.991910	0.008268	0.254756
-42.628997	-2.238455	1.996915	0.008350	0.254572
-42.314479	-2.310812	2.001920	0.008291	0.254486

-42.521509	-2.310662	2.011917	0.008330	0.254272
-42.827436	-2.300150	2.021914	0.008387	0.254014
-41.866475	-2.503059	2.031910	0.008208	0.253853
-43.025463	-2.333058	2.041907	0.008424	0.253619
-42.605400	-2.422763	2.051904	0.008346	0.253543
-42.902335	-2.414410	2.061901	0.008401	0.253282
-42.861434	-2.421808	2.071898	0.008394	0.253281
-43.208141	-2.401005	2.081894	0.008458	0.253039
-43.202618	-2.408867	2.091891	0.008457	0.252999
-43.087420	-2.429756	2.101888	0.008436	0.252999
-43.321086	-2.411384	2.111885	0.008480	0.252860
-43.414930	-2.430318	2.121882	0.008497	0.252653
-43.271952	-2.457029	2.131878	0.008471	0.252649
-43.693234	-2.376933	2.141875	0.008549	0.252668
-43.351675	-2.440854	2.151872	0.008486	0.252657
-43.329614	-2.446589	2.161869	0.008482	0.252647
-43.127876	-2.484462	2.171866	0.008444	0.252640
-43.340850	-2.444154	2.181862	0.008484	0.252648
-43.892350	-2.340808	2.191859	0.008587	0.252665
-43.621707	-2.390223	2.201856	0.008536	0.252664
-44.052673	-2.310904	2.211853	0.008617	0.252668
-43.433089	-2.425337	2.221850	0.008502	0.252658
-43.158304	-2.460734	2.231846	0.008450	0.252741
-42.549681	-2.529414	2.241843	0.008337	0.252982
-42.780005	-2.487923	2.251840	0.008380	0.252979
-42.811554	-2.482705	2.261837	0.008386	0.252975
-42.781779	-2.487093	2.271834	0.008381	0.252981
-42.532910	-2.533941	2.281830	0.008335	0.252971
-42.779974	-2.438828	2.291827	0.008381	0.253258
-42.767639	-2.436745	2.301824	0.008378	0.253282
-42.535875	-2.481576	2.311821	0.008335	0.253266
-42.071388	-2.520765	2.321818	0.008249	0.253525
-42.475780	-2.434293	2.331814	0.008324	0.253598
-42.203674	-2.481788	2.341811	0.008274	0.253609
-42.712566	-2.333872	2.351808	0.008368	0.253924
-42.046874	-2.459179	2.361805	0.008245	0.253900
-41.406366	-2.527959	2.371802	0.008126	0.254172
-42.034204	-2.399438	2.381798	0.008242	0.254252
-41.801054	-2.410818	2.391795	0.008199	0.254429
-41.569858	-2.433796	2.401792	0.008156	0.254537
-41.171249	-2.473936	2.411789	0.008082	0.254721
-41.104712	-2.460927	2.421786	0.008070	0.254863
-41.469441	-2.361215	2.431782	0.008138	0.255052
-40.965747	-2.429529	2.441779	0.008044	0.255184
-40.683100	-2.430975	2.451776	0.007992	0.255467
-40.601727	-2.435325	2.461773	0.007976	0.255526
-40.687413	-2.373629	2.471770	0.007992	0.255786
-40.309852	-2.422314	2.481766	0.007922	0.255899
-40.071297	-2.430354	2.491763	0.007878	0.256099
-39.887287	-2.426595	2.501760	0.007844	0.256309
-39.860253	-2.410514	2.511757	0.007839	0.256427
-39.545443	-2.414567	2.521754	0.007780	0.256727
-39.125802	-2.466024	2.531750	0.007702	0.256867
-38.706606	-2.517847	2.541747	0.007624	0.257004
-38.892222	-2.435745	2.551744	0.007659	0.257276
-38.698543	-2.445864	2.561741	0.007623	0.257416
-38.666780	-2.409265	2.571738	0.007617	0.257654
-38.547106	-2.382312	2.581734	0.007595	0.257928
-38.230431	-2.409887	2.591731	0.007536	0.258096
-38.081024	-2.403237	2.601728	0.007508	0.258285
-37.889467	-2.386194	2.611725	0.007473	0.258575
-37.647790	-2.398117	2.621722	0.007428	0.258754
-37.531420	-2.384790	2.631718	0.007406	0.258947
-37.097669	-2.409212	2.641715	0.007326	0.259251
-37.460167	-2.304473	2.651712	0.007393	0.259467
-36.649371	-2.417324	2.661709	0.007242	0.259660
-36.135626	-2.477639	2.671706	0.007147	0.259844
-35.930026	-2.462925	2.681702	0.007109	0.260134
-36.013357	-2.410822	2.691699	0.007124	0.260339
-35.768468	-2.420698	2.701696	0.007079	0.260531
-35.375003	-2.452500	2.711693	0.007006	0.260752
-35.704691	-2.347781	2.721690	0.007067	0.261000
-35.207346	-2.402818	2.731686	0.006974	0.261196
-34.746633	-2.452359	2.741683	0.006889	0.261385
-34.927239	-2.356732	2.751680	0.006922	0.261732
-34.508227	-2.397325	2.761677	0.006845	0.261929
-34.341410	-2.390419	2.771674	0.006814	0.262134
-34.215429	-2.370444	2.781670	0.006790	0.262371
-34.234544	-2.310947	2.791667	0.006794	0.262679
-33.488843	-2.397433	2.801664	0.006655	0.262950
-33.100141	-2.432681	2.811661	0.006583	0.263144
-33.151557	-2.387231	2.821658	0.006592	0.263343
-32.481087	-2.463223	2.831654	0.006468	0.263595
-32.398913	-2.430072	2.841651	0.006453	0.263858
-31.828491	-2.498551	2.851648	0.006346	0.264051
-31.669242	-2.491592	2.861645	0.006317	0.264248
-31.856726	-2.406026	2.871642	0.006352	0.264529
-31.576094	-2.410952	2.881638	0.006300	0.264781
-31.736596	-2.337196	2.891635	0.006330	0.265024
-31.455991	-2.341740	2.901632	0.006277	0.265278
-30.763661	-2.422059	2.911629	0.006149	0.265526
-31.271206	-2.282071	2.921626	0.006243	0.265785
-30.928585	-2.295266	2.931622	0.006180	0.266052
-30.955142	-2.241755	2.941619	0.006185	0.266317
-30.416920	-2.289473	2.951616	0.006084	0.266589
-30.231777	-2.274291	2.961613	0.006050	0.266854
-30.045124	-2.264859	2.971610	0.006015	0.267089
-29.292620	-2.348320	2.981606	0.005875	0.267378
-29.455188	-2.268844	2.991603	0.005906	0.267647
-28.717661	-2.354766	3.001600	0.005769	0.267908
-28.481414	-2.359149	3.011597	0.005725	0.268116
-29.004301	-2.213065	3.021594	0.005822	0.268390
-28.729047	-2.208191	3.031590	0.005771	0.268686
-28.177528	-2.257249	3.041587	0.005668	0.268962
-27.811566	-2.268699	3.051584	0.005600	0.269258
-27.976026	-2.192184	3.061581	0.005631	0.269508
-27.171212	-2.293482	3.071578	0.005481	0.269749
-26.757769	-2.324313	3.081574	0.005404	0.269987
-26.550098	-2.318496	3.091571	0.005366	0.270220
-26.431271	-2.274520	3.101568	0.005344	0.270571
-26.136514	-2.292116	3.111565	0.005289	0.270763
-25.929575	-2.287441	3.121562	0.005250	0.270989
-25.630845	-2.297034	3.131558	0.005195	0.271227
-25.469770	-2.279727	3.141555	0.005165	0.271475
-24.712126	-2.362904	3.151552	0.005024	0.271766
-24.680562	-2.325447	3.161549	0.005018	0.271995
-24.460902	-2.323919	3.171546	0.004977	0.272216
-24.595545	-2.250685	3.181542	0.005003	0.272474
-24.136763	-2.287898	3.191539	0.004917	0.272719
-23.733575	-2.300523	3.201536	0.004842	0.273041
-23.550136	-2.292877	3.211533	0.004808	0.273258
-23.378716	-2.278259	3.221530	0.004776	0.273500
-22.865224	-2.329810	3.231526	0.004681	0.273721
-22.466449	-2.359177	3.241523	0.004607	0.273949
-22.275511	-2.331863	3.251520	0.004571	0.274276
-22.238815	-2.299510	3.261517	0.004564	0.274481
-21.593365	-2.380655	3.271514	0.004444	0.274672
-21.644217	-2.325713	3.281510	0.004454	0.274912
-21.312940	-2.326338	3.291507	0.004392	0.275225
-21.376318	-2.265718	3.301504	0.004404	0.275483
-21.013759	-2.292470	3.311501	0.004337	0.275688
-20.867943	-2.281285	3.321498	0.004310	0.275886
-21.071302	-2.190407	3.331494	0.004348	0.276168
-20.740428	-2.195769	3.341491	0.004286	0.276455
-20.096765	-2.257225	3.351488	0.004166	0.276745
-19.806503	-2.270196	3.361485	0.004112	0.276953
-20.010623	-2.181208	3.371482	0.004150	0.277224
-19.500344	-2.227127	3.381478	0.004056	0.277468
-19.260904	-2.222213	3.391475	0.004011	0.277720
-18.930377	-2.219962	3.401472	0.003950	0.278044
-18.762095	-2.204610	3.411469	0.003918	0.278283
-18.437637	-2.214700	3.421466	0.003858	0.278537
-18.379158	-2.177783	3.431462	0.003847	0.278783
-17.432422	-2.309279	3.441459	0.003671	0.278994
-17.440689	-2.248409	3.451456	0.003673	0.279301
-17.182221	-2.249906	3.461453	0.003625	0.279537
-16.724020	-2.291741	3.471450	0.003539	0.279751
-16.293202	-2.330723	3.481446	0.003459	0.279954
-16.209641	-2.293266	3.491443	0.003444	0.280226
-15.939113	-2.287192	3.501440	0.003394	0.280511
-15.507678	-2.334087	3.511437	0.003313	0.280673
-15.617222	-2.277829	3.521434	0.003334	0.280860
-14.931942	-2.354441	3.531430	0.003206	0.281107
-14.662955	-2.356014	3.541427	0.003156	0.281350
-14.498070	-2.345919	3.551424	0.003126	0.281555
-14.554017	-2.291370	3.561421	0.003136	0.281783
-14.761907	-2.197122	3.571418	0.003175	0.282072
-14.652363	-2.161520	3.581414	0.003155	0.282357
-14.220914	-2.189819	3.591411	0.003074	0.282613
-13.801693	-2.216868	3.601408	0.002996	0.282864
-13.521738	-2.222895	3.611405	0.002944	0.283094
-13.493148	-2.179203	3.621402	0.002939	0.283343
-13.066931	-2.196403	3.631398	0.002860	0.283650
-13.042351	-2.153590	3.641395	0.002855	0.283891
-12.503874	-2.203039	3.651392	0.002755	0.284138
-12.232808	-2.206663	3.661389	0.002705	0.284370
-11.966116	-2.211996	3.671386	0.002655	0.284589
-11.851408	-2.169508	3.681382	0.002634	0.284910
-11.417758	-2.201041	3.691379	0.002553	0.285150
-11.144016	-2.204486	3.701376	0.002503	0.285385
-10.696797	-2.243436	3.711373	0.002419	0.285599
-10.412305	-2.253441	3.721370	0.002366	0.285810
-10.247363	-2.230872	3.731366	0.002336	0.286075
-9.974166	-2.240740	3.741363	0.002285	0.286276
-9.910892	-2.205948	3.751360	0.002273	0.286510
-9.553436	-2.220424	3.761357	0.002207	0.286764
-9.521960	-2.172825	3.771354	0.002201	0.287033
-9.434297	-2.139126	3.781350	0.002185	0.287283
-8.927630	-2.182601	3.791347	0.002091	0.287527
-8.250120	-2.266830	3.801344	0.001965	0.287723
-8.000619	-2.251055	3.811341	0.001918	0.288029
-7.860848	-2.232523	3.821338	0.001892	0.288250
-7.624794	-2.237418	3.831334	0.001848	0.288440
-7.360679	-2.240998	3.841331	0.001799	0.288663
-6.886554	-2.269066	3.851328	0.001711	0.288953
-6.303338	-2.334651	3.861325	0.001603	0.289155
-6.288521	-2.303624	3.871322	0.001600	0.289324
-5.871051	-2.329561	3.881318	0.001522	0.289573
-5.723385	-2.311999	3.891315	0.001495	0.289794
-6.014728	-2.215075	3.901312	0.001549	0.290013
-6.042081	-2.162687	3.911309	0.001554	0.290249
-5.363463	-2.223395	3.921306	0.001428	0.290561
-5.129757	-2.230063	3.931302	0.001385	0.290739
-4.782185	-2.256995	3.941299	0.001320	0.290919
-4.322648	-2.302240	3.951296	0.001235	0.291109
-4.395068	-2.227097	3.961293	0.001248	0.291416
-3.803911	-2.294351	3.971290	0.001138	0.291616
-4.174044	-2.181573	3.981286	0.001207	0.291841
-4.220480	-2.124876	3.991283	0.001216	0.292080
-3.063159	-2.280355	4.001280	0.001001	0.292351
-3.142324	-2.221372	4.011277	0.001015	0.292571
-3.222153	-2.158883	4.021274	0.001030	0.292808
-3.042277	-2.140329	4.031270	0.000997	0.293061
-2.452994	-2.199530	4.041267	0.000887	0.293297
-2.328128	-2.166554	4.051264	0.000864	0.293571
-2.625648	-2.064063	4.061261	0.000920	0.293809
-2.216447	-2.086813	4.071258	0.000843	0.294063
-2.240958	-2.027435	4.081254	0.000848	0.294332
-2.506718	-1.922143	4.091251	0.000898	0.294612
-1.665767	-2.019687	4.101248	0.000741	0.294883
-1.653412	-1.956832	4.111245	0.000739	0.295202
-1.581672	-1.907015	4.121242	0.000726	0.295510
-1.525656	-1.869865	4.131238	0.000715	0.295741
-1.759744	-1.766610	4.141235	0.000759	0.296037
-1.595379	-1.734595	4.151232	0.000728	0.296339
-1.248472	-1.730935	4.161229	0.000664	0.296664
-1.343616	-1.649107	4.171226	0.000682	0.296979
-1.073794	-1.631701	4.181222	0.000631	0.297302
-0.587573	-1.654352	4.191219	0.000541	0.297621
-0.688344	-1.566659	4.201216	0.000560	0.297958
-0.835890	-1.473710	4.211213	0.000587	0.298278
-1.103232	-1.349104	4.221210	0.000637	0.298646
-0.764100	-1.331469	4.231206	0.000574	0.299030
-0.400654	-1.323782	4.241203	0.000506	0.299386
-0.596741	-1.214281	4.251200	0.000543	0.299742
-0.540135	-1.146013	4.261197	0.000532	0.300121
-0.533016	-1.062785	4.271194	0.000531	0.300528
-0.019772	-1.083013	4.281190	0.000436	0.300879
0.475406	-1.100432	4.291187	0.000344	0.301227
0.526179	-1.031593	4.301184	0.000334	0.301601
0.195000	-0.893312	4.311181	0.000396	0.301975
0.084637	-0.776558	4.321178	0.000416	0.302438
0.107903	-0.691866	4.331174	0.000412	0.302863
0.107533	-0.605850	4.341171	0.000412	0.303273
0.223129	-0.524957	4.351168	0.000391	0.303758
0.310360	-0.452121	4.361165	0.000375	0.304180
0.906764	-0.466983	4.371162	0.000264	0.304624
0.753064	-0.346875	4.381158	0.000292	0.305061
0.630174	-0.218439	4.391155	0.000315	0.305563
0.330368	-0.072686	4.401152	0.000371	0.305995
0.000000	0.081033	4.411149	0.000432	0.306437

0.161256	0.322946	4.416154	0.000402	0.307715
0.251770	0.860604	4.421158	0.000385	0.310309
0.717155	1.611711	4.426163	0.000298	0.314182
1.334197	2.624340	4.431168	0.000183	0.319319
1.772677	3.955586	4.436173	0.000100	0.325649
2.460635	5.543584	4.441178	-0.000029	0.333173
2.518294	7.541461	4.446182	-0.000041	0.341783
3.056920	9.766186	4.451187	-0.000143	0.351477
3.714971	12.268013	4.456192	-0.000267	0.362107
4.374772	15.091044	4.461197	-0.000391	0.373680
5.135088	18.229138	4.466202	-0.000535	0.386155
5.627630	21.754882	4.471206	-0.000629	0.399469
6.850308	25.489428	4.476211	-0.000859	0.413548
8.057886	29.578965	4.481216	-0.001087	0.428354
8.863734	34.088659	4.486221	-0.001239	0.443799
9.146853	39.059013	4.491226	-0.001295	0.459876
9.985177	44.264069	4.496230	-0.001455	0.476428
10.692991	49.851792	4.501235	-0.001590	0.493477
11.415512	55.782978	4.506240	-0.001729	0.510937
12.399521	61.986680	4.511245	-0.001916	0.528694
14.350594	68.357350	4.516250	-0.002283	0.546776
14.833616	75.306462	4.521254	-0.002378	0.565083
15.317081	82.565258	4.526259	-0.002472	0.583582
17.036335	89.887315	4.531264	-0.002797	0.602198
20.763427	97.140958	4.536269	-0.003496	0.620933
21.890166	105.144513	4.541274	-0.003711	0.639759
22.264715	113.515473	4.546278	-0.003786	0.658557
23.525749	121.942891	4.551283	-0.004026	0.677291
24.436829	130.620324	4.556288	-0.004201	0.695910
24.625901	139.599341	4.561293	-0.004242	0.714393
27.794360	148.198282	4.566298	-0.004838	0.732706
29.097481	157.310987	4.571302	-0.005087	0.750921
29.985939	166.603920	4.576307	-0.005258	0.768903
31.163988	175.950813	4.581312	-0.005483	0.786667
31.315990	185.562118	4.586317	-0.005518	0.804186
32.236841	195.094935	4.591322	-0.005696	0.821433
33.261945	204.664052	4.596326	-0.005893	0.838419
34.375996	214.238066	4.601331	-0.006106	0.855101
35.195264	223.894041	4.606336	-0.006265	0.871513
35.953428	233.560222	4.611341	-0.006412	0.887620
37.849713	243.050556	4.616346	-0.006772	0.903478
39.216324	252.633503	4.621350	-0.007032	0.919060
39.853900	262.319371	4.626355	-0.007157	0.934343
41.375803	271.828811	4.631360	-0.007447	0.949347
42.316693	281.401787	4.636365	-0.007628	0.964059
43.548251	290.919192	4.641370	-0.007864	0.978542
43.718418	300.600811	4.646374	-0.007902	0.992782
44.536428	310.071557	4.651379	-0.008060	1.006681
47.059748	319.222273	4.656384	-0.008536	1.020356
48.123476	328.594498	4.661389	-0.008740	1.033804
49.118669	337.939170	4.666394	-0.008931	1.047024
49.473470	347.343436	4.671398	-0.009003	1.060008
50.971949	356.494304	4.676403	-0.009288	1.072761
52.323288	365.627576	4.681408	-0.009546	1.085305
54.317220	374.618498	4.686413	-0.009923	1.097664
55.367081	383.751884	4.691418	-0.010124	1.109858
56.599251	392.789308	4.696422	-0.010360	1.121835
57.290468	401.897327	4.701427	-0.010494	1.133656
58.135111	410.933141	4.706432	-0.010657	1.145298
59.038991	419.901258	4.711437	-0.010832	1.156750
59.895031	428.817295	4.716442	-0.010997	1.168014
60.712502	437.706717	4.721446	-0.011155	1.179130
61.133914	446.631649	4.726451	-0.011239	1.190102
62.084211	455.427453	4.731456	-0.011422	1.200928
63.306191	464.124146	4.736461	-0.011655	1.211592
64.191020	472.885661	4.741466	-0.011825	1.222173
65.338960	481.555365	4.746470	-0.012044	1.232606
65.909339	490.273374	4.751475	-0.012156	1.242894
66.202814	499.038214	4.756480	-0.012217	1.253097
66.296986	507.767623	4.761485	-0.012240	1.263138
66.959475	516.381698	4.766490	-0.012369	1.273078
68.901686	524.732372	4.771494	-0.012736	1.282887
70.787050	533.137161	4.776499	-0.013092	1.292671
72.589968	541.582159	4.781504	-0.013433	1.302410
73.074091	550.265983	4.786509	-0.013529	1.312094
73.670421	558.860121	4.791514	-0.013646	1.321629
74.110743	567.393159	4.796518	-0.013733	1.331002
74.330015	575.964338	4.801523	-0.013780	1.340309
74.498029	584.535916	4.806528	-0.013816	1.349544
75.553099	592.880794	4.811533	-0.014018	1.358633
75.990138	601.360292	4.816538	-0.014105	1.367694
76.568493	609.779377	4.821542	-0.014218	1.376656
76.617766	618.293738	4.826547	-0.014233	1.385567
77.451390	626.670002	4.831552	-0.014394	1.394414
78.117423	635.012764	4.836557	-0.014523	1.403142
79.232632	643.308869	4.841562	-0.014736	1.411843
79.660919	651.714091	4.846566	-0.014821	1.420486
80.467488	660.046848	4.851571	-0.014977	1.429067
80.970512	668.435251	4.856576	-0.015076	1.437602
81.510479	676.751598	4.861581	-0.015182	1.446020
81.826257	685.156883	4.866586	-0.015246	1.454441
83.160956	693.348140	4.871590	-0.015500	1.462767
83.397565	701.775060	4.876595	-0.015549	1.471100
83.218781	710.222441	4.881600	-0.015521	1.479339
84.561861	718.354241	4.886605	-0.015777	1.487469
85.239221	726.656799	4.891610	-0.015908	1.495614
86.251944	734.866334	4.896614	-0.016102	1.503677
87.575488	743.044702	4.901619	-0.016354	1.511716
87.970566	751.394625	4.906624	-0.016433	1.519731
88.929051	759.595118	4.911629	-0.016617	1.527649
88.818434	768.042568	4.916634	-0.016601	1.535594
89.038855	776.367730	4.921638	-0.016648	1.543435
89.810290	784.592573	4.926643	-0.016797	1.551226
91.386644	792.689935	4.931648	-0.017096	1.558980
91.395512	801.053058	4.936653	-0.017103	1.566707
92.157777	809.285418	4.941658	-0.017250	1.574387
92.882713	817.487152	4.946662	-0.017390	1.581996
93.567754	825.728347	4.951667	-0.017523	1.589599
93.943480	834.034517	4.956672	-0.017598	1.597178
94.072177	842.323246	4.961677	-0.017628	1.604671
94.551822	850.576186	4.966682	-0.017722	1.612147
94.825749	858.827527	4.971686	-0.017779	1.619557
95.566778	867.015891	4.976691	-0.017922	1.626944
96.435756	875.216392	4.981696	-0.018089	1.634326
97.154589	883.357595	4.986701	-0.018228	1.641602
98.193440	891.489979	4.991706	-0.018427	1.648882
99.350754	899.605320	4.996710	-0.018648	1.656132
99.590299	907.897007	5.001715	-0.018698	1.663375
100.062091	916.147889	5.006720	-0.018791	1.670584
100.826825	924.318717	5.011725	-0.018938	1.677733
101.883337	932.435201	5.016730	-0.019140	1.684844
102.393193	940.671665	5.021734	-0.019241	1.691953
102.960908	948.863448	5.026739	-0.019352	1.699003
102.996278	957.158620	5.031744	-0.019364	1.706039
103.068689	965.435762	5.036749	-0.019382	1.713036
103.808863	973.550332	5.041754	-0.019526	1.719956
104.642424	981.667427	5.046758	-0.019686	1.726863
105.023978	989.891508	5.051763	-0.019762	1.733772
105.918881	998.009197	5.056768	-0.019934	1.740633
106.736086	1006.136527	5.061773	-0.020092	1.747463
106.771686	1014.425730	5.066778	-0.020104	1.754300
107.176976	1022.593624	5.071782	-0.020184	1.761057
107.642565	1030.768033	5.076787	-0.020276	1.767802
108.079294	1038.957942	5.081792	-0.020363	1.774530
109.148014	1047.007007	5.086797	-0.020567	1.781198
109.644778	1055.204291	5.091802	-0.020665	1.787889
110.277876	1063.383250	5.096806	-0.020788	1.794557
111.140799	1071.476114	5.101811	-0.020954	1.801159
112.083437	1079.578374	5.106816	-0.021135	1.807755
112.828876	1087.719164	5.111821	-0.021279	1.814332
113.827723	1095.828955	5.116826	-0.021470	1.820892
114.068270	1104.070012	5.121830	-0.021520	1.827440
114.597678	1112.240924	5.126835	-0.021624	1.833943
114.774866	1120.481554	5.131840	-0.021662	1.840436
115.782007	1128.515552	5.136845	-0.021855	1.846844
116.256695	1136.710257	5.141850	-0.021949	1.853291
116.899892	1144.837055	5.146854	-0.022074	1.859683
118.104802	1152.856593	5.151859	-0.022303	1.866037
119.079129	1160.988358	5.156864	-0.022490	1.872428
120.104224	1169.053851	5.161869	-0.022686	1.878752
120.915810	1177.180726	5.166874	-0.022842	1.885076
121.459151	1185.367597	5.171878	-0.022949	1.891394
121.654838	1193.611326	5.176883	-0.022991	1.897693
122.046961	1201.780019	5.181888	-0.023069	1.903937
122.134382	1209.990394	5.186893	-0.023090	1.910157
122.992502	1218.067079	5.191898	-0.023255	1.916345
123.845843	1226.135594	5.196902	-0.023420	1.922505
123.959312	1234.355120	5.201907	-0.023446	1.928675
124.723887	1242.466614	5.206912	-0.023594	1.934818
125.285183	1250.564913	5.211917	-0.023703	1.940908
126.265173	1258.654041	5.216922	-0.023891	1.947020
127.406460	1266.692745	5.221926	-0.024109	1.953092
127.873928	1274.835519	5.226931	-0.024201	1.959148
128.443278	1282.949258	5.231936	-0.024312	1.965174
128.682925	1291.133189	5.236941	-0.024362	1.971197
129.150000	1299.305952	5.241946	-0.024455	1.977219
129.432178	1307.438341	5.246950	-0.024512	1.983172
129.274299	1315.672603	5.251955	-0.024488	1.989134
129.775050	1323.785872	5.256960	-0.024587	1.995062
130.656431	1331.777314	5.261965	-0.024756	2.000925
131.718456	1339.778227	5.266970	-0.024959	2.006796
131.656632	1348.016726	5.271974	-0.024953	2.012701
131.846451	1356.155286	5.276979	-0.024993	2.018544
132.078621	1364.304972	5.281984	-0.025042	2.024382
132.241667	1372.439404	5.286989	-0.025077	2.030185
132.900481	1380.509196	5.291994	-0.025205	2.035978
133.818731	1388.524658	5.296998	-0.025381	2.041743
134.145465	1396.644118	5.302003	-0.025448	2.047504
134.028638	1404.878503	5.307008	-0.025431	2.053282
134.455821	1412.947898	5.312013	-0.025516	2.058986
135.070436	1420.995959	5.317018	-0.025636	2.064677
135.666228	1429.073983	5.322022	-0.025752	2.070372
136.222518	1437.146366	5.327027	-0.025860	2.076043
136.600086	1445.274415	5.332032	-0.025936	2.081719
137.147657	1453.338212	5.337037	-0.026043	2.087352
137.791136	1461.436762	5.342042	-0.026168	2.093003
138.378191	1469.525733	5.347046	-0.026283	2.098627
138.519485	1477.677359	5.352051	-0.026314	2.104233
139.600148	1485.719856	5.357056	-0.026521	2.109844
140.332387	1493.811131	5.362061	-0.026662	2.115438
141.039919	1501.861626	5.367066	-0.026799	2.120988
141.553334	1509.971990	5.372070	-0.026900	2.126544
141.568538	1518.163968	5.377075	-0.026908	2.132092
142.322523	1526.206129	5.382080	-0.027054	2.137596
142.756996	1534.292221	5.387085	-0.027140	2.143085
143.553194	1542.377115	5.392090	-0.027293	2.148593
143.958316	1550.495503	5.397094	-0.027374	2.154072
144.437438	1558.564637	5.402099	-0.027469	2.159512
144.875546	1566.663888	5.407104	-0.027555	2.164953
145.468300	1574.741520	5.412109	-0.027671	2.170382
145.871893	1582.855327	5.417114	-0.027751	2.175802
146.063987	1590.980428	5.422118	-0.027792	2.181197
146.550349	1599.046924	5.427123	-0.027888	2.186567
146.807244	1607.183379	5.432128	-0.027941	2.191948
147.121024	1615.246289	5.437133	-0.028005	2.197274
147.676931	1623.301079	5.442138	-0.028114	2.202603
147.681514	1631.454904	5.447142	-0.028120	2.207933
147.790861	1639.583423	5.452147	-0.028145	2.213243
148.828017	1647.545156	5.457152	-0.028344	2.218518
148.949506	1655.655374	5.462157	-0.028371	2.223792
149.563942	1663.743228	5.467162	-0.028491	2.229084
149.537963	1671.890093	5.472166	-0.028491	2.234343
149.683626	1679.983755	5.477171	-0.028524	2.239572
150.009952	1688.073523	5.482176	-0.028590	2.244801
150.207453	1696.165861	5.487181	-0.028632	2.250009
150.525457	1704.249488	5.492186	-0.028696	2.255210
150.651168	1712.350988	5.497190	-0.028725	2.260393
151.797157	1720.273812	5.502195	-0.028943	2.265541
152.227873	1728.430280	5.507200	-0.029029	2.270762
152.418972	1736.528761	5.512205	-0.029070	2.275913
153.218886	1744.510225	5.517210	-0.029224	2.281032
153.548785	1752.574688	5.522214	-0.029290	2.286151
154.120686	1760.618469	5.527219	-0.029402	2.291266
154.482296	1768.739841	5.532224	-0.029475	2.296400
154.767664	1776.821389	5.537229	-0.029533	2.301491
155.290050	1784.902325	5.542234	-0.029636	2.306590
155.574585	1792.997493	5.547238	-0.029694	2.311667
156.225354	1801.011586	5.552243	-0.029820	2.316713
156.772355	1809.088558	5.557248	-0.029927	2.321779
157.431981	1817.132066	5.562253	-0.030055	2.326822
158.261634	1825.157061	5.567258	-0.030215	2.331857
158.221543	1833.331391	5.572262	-0.030213	2.336900
158.839228	1841.355610	5.577267	-0.030333	2.341894
159.191588	1849.492576	5.582272	-0.030404	2.346925
159.124215	1857.639723	5.587277	-0.030396	2.351917
159.917696	1865.621420	5.592282	-0.030549	2.356868
160.311101	1873.681961	5.597286	-0.030628	2.361823
160.942878	1881.695583	5.602291	-0.030751	2.366760
161.059187	1889.848607	5.607296	-0.030778	2.371728
161.713347	1897.863423	5.612301	-0.030905	2.376646
161.769957	1906.010567	5.617306	-0.030920	2.381584
162.581986	1913.988514	5.622310	-0.031077	2.386472
162.142561	1922.231948	5.627315	-0.031000	2.391409
162.120091	1930.349355	5.632320	-0.031001	2.396293
162.749177	1938.308691	5.637325	-0.031124	2.401124
163.190561	1946.343799	5.642330	-0.031211	2.405977
163.641631	1954.422343	5.647334	-0.031300	2.410846
164.002685	1962.489258	5.652339	-0.031373	2.415691
164.154644	1970.580336	5.657344	-0.031406	2.420524
164.539185	1978.609660	5.662349	-0.031483	2.425329
165.396610	1986.634361	5.667354	-0.031648	2.430159
165.529714	1994.782942	5.672358	-0.031678	2.434995
166.454048	2002.725723	5.677363	-0.031855	2.439763
166.879402	2010.793676	5.682368	-0.031939	2.444556
167.449219	2018.822545	5.687373	-0.032051	2.449327
167.949205	2026.900078	5.692378	-0.032149	2.454112
169.002976	2034.897484	5.697382	-0.032350	2.458884
169.514984	2042.957385	5.702387	-0.032451	2.463641
170.190447	2051.034444	5.707392	-0.032582	2.468411
170.605415	2059.109526	5.712397	-0.032664	2.473151
170.867566	2067.233841	5.717402	-0.032718	2.477899
171.538784	2075.243957	5.722406	-0.032849	2.482602
172.437857	2083.263098	5.727411	-0.033021	2.487319
173.093566	2091.340617	5.732416	-0.033149	2.492042
172.912998	2099.526380	5.737421	-0.033120	2.496755
173.443738	2107.552260	5.742426	-0.033224	2.501421
173.907609	2115.603792	5.747430	-0.033316	2.506088
174.155525	2123.715797	5.752435	-0.033367	2.510764
174.896789	2131.713485	5.757440	-0.033510	2.515403
175.073518	2139.804627	5.762445	-0.033549	2.520045
174.867244	2147.932366	5.767450	-0.033515	2.524671
175.491972	2155.916469	5.772454	-0.033637	2.529268
175.958362	2163.948244	5.777459	-0.033729	2.533872
176.272161	2172.073147	5.782464	-0.033793	2.538509
176.689178	2180.067840	5.787469	-0.033875	2.543072
176.932755	2188.143292	5.792474	-0.033926	2.547659
177.527803	2196.171606	5.797478	-0.034042	2.552236
177.591359	2204.303134	5.802483	-0.034059	2.556826
178.048294	2212.330007	5.807488	-0.034149	2.561376
178.212828	2220.406191	5.812493	-0.034185	2.565925
179.136011	2228.381935	5.817498	-0.034362	2.570463
179.331238	2236.498854	5.822502	-0.034404	2.575021
179.397166	2244.551337	5.827507	-0.034421	2.579525
179.534733	2252.660130	5.832512	-0.034452	2.584058
179.854411	2260.703278	5.837517	-0.034517	2.588560
180.378999	2268.824992	5.842522	-0.034620	2.593111
181.341715	2276.770947	5.847526	-0.034804	2.597588
181.390248	2284.849329	5.852531	-0.034818	2.602066
181.852487	2292.902974	5.857536	-0.034910	2.606551
181.451820	2301.068543	5.862541	-0.034840	2.611031
181.959293	2309.091647	5.867546	-0.034940	2.615488
182.376753	2317.094566	5.872550	-0.035023	2.619919
182.629047	2325.112002	5.877555	-0.035075	2.624339
183.049707	2333.173706	5.882560	-0.035159	2.628788
183.274944	2341.242252	5.887565	-0.035206	2.633220
183.726264	2349.260416	5.892570	-0.035295	2.637631
184.116563	2357.276370	5.897574	-0.035373	2.642030
184.568168	2365.310667	5.902579	-0.035462	2.646436
185.255026	2373.335862	5.907584	-0.035595	2.650845
185.725044	2381.378871	5.912589	-0.035688	2.655242
185.922168	2389.466548	5.917594	-0.035730	2.659638
186.815585	2397.432358	5.922598	-0.035901	2.664006
187.239364	2405.516356	5.927603	-0.035985	2.668400
187.886099	2413.586588	5.932608	-0.036111	2.672794
188.340405	2421.631372	5.937613	-0.036201	2.677154
188.440612	2429.717733	5.942618	-0.036225	2.681506
188.407945	2437.814304	5.947622	-0.036224	2.685848
189.053594	2445.813281	5.952627	-0.036349	2.690175
189.186232	2453.915419	5.957632	-0.036379	2.694516
189.317992	2461.984000	5.962637	-0.036409	2.698833
190.217476	2469.923216	5.967642	-0.036582	2.703123
190.678383	2478.005604	5.972646	-0.036673	2.707454
190.872216	2486.075293	5.977651	-0.036714	2.711755
191.360255	2494.111794	5.982656	-0.036810	2.716049
191.806271	2502.129799	5.987661	-0.036898	2.720325
192.002360	2510.202575	5.992666	-0.036940	2.724606
192.216635	2518.262908	5.997670	-0.036985	2.728875
192.213772	2526.369745	6.002675	-0.036990	2.733149
192.474640	2534.426234	6.007680	-0.037044	2.737406
192.458378	2542.502988	6.012685	-0.037046	2.741649
192.814169	2550.524029	6.017690	-0.037117	2.745880
193.634286	2558.515448	6.022694	-0.037275	2.750118
194.091265	2566.574819	6.027699	-0.037365	2.754362
194.355413	2574.611165	6.032704	-0.037420	2.758575
194.606140	2582.642376	6.037709	-0.037472	2.762779
195.091975	2590.649737	6.042714	-0.037567	2.766978
195.566344	2598.718381	6.047718	-0.037661	2.771202
196.037845	2606.753005	6.052723	-0.037754	2.775401
196.524376	2614.804935	6.057728	-0.037850	2.779604
196.363784	2622.923697	6.062733	-0.037825	2.783795
196.706515	2630.941106	6.067738	-0.037894	2.787959
197.148997	2638.999585	6.072742	-0.037981	2.792143
197.536174	2647.020480	6.077747	-0.038059	2.796299
198.076587	2655.041100	6.082752	-0.038165	2.800457
198.494700	2663.059626	6.087757	-0.038248	2.804600
199.147711	2671.076921	6.092762	-0.038374	2.808751
199.112151	2679.225521	6.097766	-0.038373	2.812922
199.365992	2687.268919	6.102771	-0.038425	2.817050
199.737185	2695.313119	6.107776	-0.038500	2.821179
200.019256	2703.322635	6.112781	-0.038557	2.825279
200.521308	2711.341265	6.117786	-0.038656	2.829391
200.801084	2719.444787	6.122790	-0.038713	2.833526
201.010403	2727.457628	6.127795	-0.038758	2.837606
201.601590	2735.474019	6.132800	-0.038873	2.841704
201.888558	2743.498924	6.137805	-0.038932	2.845782
202.266345	2751.564059	6.142810	-0.039007	2.849880
202.950904	2759.546538	6.147814	-0.039140	2.853948
203.475161	2767.564658	6.152819	-0.039242	2.858019
204.077431	2775.625360	6.157824	-0.039360	2.862109
204.381587	2783.687058	6.162829	-0.039422	2.866178
204.844301	2791.721224	6.167834	-0.039513	2.870235
204.886269	2799.856459	6.172838	-0.039526	2.874314
204.945852	2807.906378	6.177843	-0.039542	2.878345
205.060544	2815.960151	6.182848	-0.039569	2.882376
205.667565	2823.928460	6.187853	-0.039687	2.886385
206.038056	2832.012551	6.192858	-0.039761	2.890434
206.303443	2840.080432	6.197862	-0.039816	2.894463
206.307316	2848.115455	6.202867	-0.039822	2.898455
206.938156	2856.131071	6.207872	-0.039945	2.902467
207.568190	2864.119128	6.212877	-0.040067	2.906460
207.947714	2872.193180	6.217882	-0.040143	2.910476
208.420896	2880.252998	6.222886	-0.040236	2.914484
208.517950	2888.308355	6.227891	-0.040259	2.918464
209.198760	2896.276410	6.232896	-0.040391	2.922428
209.676656	2904.302888	6.237901	-0.040486	2.926403
210.395066	2912.299340	6.242906	-0.040624	2.930372
210.211735	2920.470189	6.247910	-0.040596	2.934371
210.507614	2928.460335	6.252915	-0.040656	2.938303
210.689891	2936.568318	6.257920	-0.040695	2.942281
211.027158	2944.571287	6.262925	-0.040763	2.946210
211.627642	2952.573574	6.267930	-0.040880	2.950148
212.026238	2960.648060	6.272934	-0.040959	2.954104
212.284856	2968.677633	6.277939	-0.041013	2.958027
212.497224	2976.721120	6.282944	-0.041058	2.961948
212.679869	2984.768968	6.287949	-0.041097	2.965864
213.161288	2992.769343	6.292954	-0.041192	2.969768
213.643789	3000.808784	6.297958	-0.041287	2.973686
213.648276	3008.859119	6.302963	-0.041293	2.977579
213.953346	3016.936706	6.307968	-0.041355	2.981496
214.646491	3024.898391	6.312973	-0.041489	2.985371
214.692558	3033.007881	6.317978	-0.041503	2.989279
215.719476	3040.945381	6.322982	-0.041699	2.993150
216.388214	3048.937960	6.327987	-0.041829	2.997024
216.388719	3057.070706	6.332992	-0.041834	3.000926
216.767758	3065.032769	6.337997	-0.041910	3.004760
216.899537	3073.163453	6.343002	-0.041940	3.008657
216.911470	3081.290708	6.348006	-0.041947	3.012541
217.492165	3089.235825	6.353011	-0.042060	3.016363
218.204508	3097.218005	6.358016	-0.042198	3.020204
218.705513	3105.225220	6.363021	-0.042297	3.024040
219.218729	3113.254070	6.368026	-0.042397	3.027883
219.561717	3121.373852	6.373030	-0.042466	3.031756
219.888275	3129.389986	6.378035	-0.042532	3.035573
220.561836	3137.381916	6.383040	-0.042663	3.039392
220.690461	3145.440734	6.388045	-0.042692	3.043210
221.227876	3153.464320	6.393050	-0.042797	3.047027
221.754146	3161.532526	6.398054	-0.042901	3.050860
221.881741	3169.601016	6.403059	-0.042930	3.054668
222.335368	3177.633771	6.408064	-0.043019	3.058471
222.556506	3185.694270	6.413069	-0.043066	3.062270
223.065451	3193.697132	6.418074	-0.043166	3.066052
223.374733	3201.768785	6.423078	-0.043228	3.069851
223.217203	3209.910829	6.428083	-0.043204	3.073656
223.411744	3217.935754	6.433088	-0.043246	3.077419
224.063718	3225.864021	6.438093	-0.043372	3.081154
223.883713	3233.945277	6.443098	-0.043344	3.084915
224.599520	3241.914319	6.448102	-0.043482	3.088663
224.722566	3249.950033	6.453107	-0.043510	3.092409
225.313918	3257.994110	6.458112	-0.043626	3.096176
225.634006	3265.995201	6.463117	-0.043690	3.099906
225.536082	3274.087020	6.468122	-0.043677	3.103654
226.028704	3282.094221	6.473126	-0.043774	3.107385
226.291223	3290.146779	6.478131	-0.043828	3.111123
227.138730	3298.085769	6.483136	-0.043991	3.114830
227.047107	3306.181576	6.488141	-0.043980	3.118562
227.368342	3314.195295	6.493146	-0.044045	3.122271
227.931299	3322.234443	6.498150	-0.044155	3.125998
228.254210	3330.233518	6.503155	-0.044220	3.129691
228.819719	3338.307019	6.508160	-0.044330	3.133425
228.572770	3346.416499	6.513165	-0.044290	3.137133
229.251730	3354.389221	6.518170	-0.044421	3.140817
229.907495	3362.356900	6.523174	-0.044548	3.144494
229.874542	3370.471707	6.528179	-0.044548	3.148201
230.082609	3378.542746	6.533184	-0.044592	3.151896
230.773173	3386.523547	6.538189	-0.044725	3.155566
230.977887	3394.557191	6.543194	-0.044769	3.159234
231.921459	3402.519886	6.548198	-0.044949	3.162899
231.913905	3410.601008	6.553203	-0.044953	3.166571
232.554473	3418.621676	6.558208	-0.045078	3.170240
232.713965	3426.708759	6.563213	-0.045113	3.173913
232.803217	3434.766638	6.568218	-0.045134	3.177566
233.605573	3442.738682	6.573222	-0.045289	3.181207
233.754733	3450.776293	6.578227	-0.045322	3.184845
234.104270	3458.832771	6.583232	-0.045392	3.188496
234.747939	3466.820922	6.588237	-0.045517	3.192125
234.875617	3474.895512	6.593242	-0.045546	3.195766
235.239157	3482.910746	6.598246	-0.045619	3.199386
235.308630	3490.960823	6.603251	-0.045637	3.203005
235.425515	3499.028015	6.608256	-0.045664	3.206630
235.523872	3507.074119	6.613261	-0.045688	3.210240
235.901379	3515.058619	6.618266	-0.045763	3.213830
236.652582	3523.064698	6.623270	-0.045908	3.217443
237.544454	3531.000290	6.628275	-0.046079	3.221025
237.539109	3539.139161	6.633280	-0.046084	3.224656
237.662594	3547.199259	6.638285	-0.046112	3.228253
237.728046	3555.252870	6.643290	-0.046129	3.231841
238.168537	3563.273640	6.648294	-0.046216	3.235426
238.098687	3571.308847	6.653299	-0.046209	3.238992
238.654627	3579.294584	6.658304	-0.046317	3.242558
239.086197	3587.311668	6.663309	-0.046403	3.246129
239.223105	3595.354177	6.668314	-0.046434	3.249695
239.372282	3603.409389	6.673318	-0.046467	3.253263
239.470661	3611.464132	6.678323	-0.046490	3.256825
239.874693	3619.475158	6.683328	-0.046570	3.260376
239.775798	3627.537700	6.688333	-0.046557	3.263926
240.146933	3635.531245	6.693338	-0.046632	3.267460
240.362941	3643.609103	6.698342	-0.046677	3.271021
240.709266	3651.565073	6.703347	-0.046747	3.274531
241.102013	3659.596649	6.708352	-0.046825	3.278071
241.479052	3667.639980	6.713357	-0.046900	3.281612
241.675429	3675.660291	6.718362	-0.046942	3.285132
241.837168	3683.711766	6.723366	-0.046977	3.288660
242.292852	3691.695733	6.728371	-0.047067	3.292166
242.747802	3699.777255	6.733376	-0.047157	3.295712
243.187990	3707.720029	6.738381	-0.047244	3.299192
243.569504	3715.749906	6.743386	-0.047321	3.302704
243.515591	3723.894821	6.748390	-0.047316	3.306246
243.306928	3731.979087	6.753395	-0.047282	3.309751
243.331982	3740.032718	6.758400	-0.047292	3.313248
243.939833	3747.962366	6.763405	-0.047410	3.316711
244.102256	3756.005580	6.768410	-0.047446	3.320201
244.735525	3763.948658	6.773414	-0.047569	3.323663
244.770992	3772.021091	6.778419	-0.047581	3.327154
245.878810	3779.988798	6.783424	-0.047792	3.330638
245.867932	3788.061563	6.788429	-0.047795	3.334120
245.866843	3796.129575	6.793434	-0.047800	3.337597
246.527758	3804.153015	6.798438	-0.047929	3.341076
246.975256	3812.125609	6.803443	-0.048017	3.344521
246.992523	3820.255941	6.808448	-0.048026	3.348014
247.384768	3828.280899	6.813453	-0.048104	3.351473
247.642516	3836.267161	6.818458	-0.048157	3.354906
247.829391	3844.345277	6.823462	-0.048197	3.358373
248.426187	3852.274703	6.828467	-0.048313	3.361787
248.759367	3860.326168	6.833472	-0.048380	3.365240
248.838993	3868.379658	6.838477	-0.048400	3.368681
249.658360	3876.364579	6.843482	-0.048558	3.372117
249.605808	3884.510028	6.848486	-0.048554	3.375585
249.795641	3892.476226	6.853491	-0.048594	3.378983
250.017584	3900.505067	6.858496	-0.048641	3.382405
250.691147	3908.492894	6.863501	-0.048771	3.385822
250.917765	3916.540841	6.868506	-0.048819	3.389245
251.455489	3924.603485	6.873510	-0.048924	3.392682
251.315447	3932.692807	6.878515	-0.048903	3.396102
251.980990	3940.629053	6.883520	-0.049032	3.399483
252.043221	3948.690027	6.888525	-0.049049	3.402892
252.493450	3956.697986	6.893530	-0.049138	3.406288
253.064217	3964.691334	6.898534	-0.049249	3.409680
253.747595	3972.681898	6.903539	-0.049382	3.413071
254.088328	3980.731219	6.908544	-0.049450	3.416471
253.822676	3988.824993	6.913549	-0.049406	3.419864
254.177843	3996.814976	6.918554	-0.049478	3.423233
254.331162	4004.914058	6.923558	-0.049511	3.426637
254.405813	4012.929504	6.928563	-0.049530	3.429999
254.944769	4020.939433	6.933568	-0.049636	3.433373
254.893141	4029.030609	6.938573	-0.049632	3.436756
254.848884	4037.036460	6.943578	-0.049628	3.440101
255.542379	4044.980664	6.948582	-0.049763	3.443442
255.916380	4052.993800	6.953587	-0.049838	3.446797
256.063711	4061.059874	6.958592	-0.049870	3.450164
256.518071	4069.077855	6.963597	-0.049960	3.453518
256.728579	4077.117879	6.968602	-0.050004	3.456869
257.250584	4085.090663	6.973606	-0.050107	3.460199
257.144415	4093.173163	6.978611	-0.050092	3.463551
258.030117	4101.142615	6.983616	-0.050262	3.466886
258.280881	4109.200485	6.988621	-0.050314	3.470232
258.592552	4117.229618	6.993626	-0.050377	3.473566
259.031466	4125.297104	6.998630	-0.050464	3.476917
259.106053	4133.285576	7.003635	-0.050483	3.480219
259.546793	4141.295306	7.008640	-0.050571	3.483539
259.772870	4149.333181	7.013645	-0.050618	3.486861
259.981993	4157.402183	7.018650	-0.050662	3.490191
259.745904	4165.507789	7.023654	-0.050623	3.493519
260.676002	4173.382824	7.028659	-0.050802	3.496787
261.020399	4181.433216	7.033664	-0.050871	3.500105
261.272365	4189.462217	7.038669	-0.050923	3.503408
261.335745	4197.501670	7.043674	-0.050940	3.506706
262.457309	4205.449078	7.048678	-0.051154	3.509997
262.586450	4213.532335	7.053683	-0.051183	3.513308
263.057057	4221.564340	7.058688	-0.051276	3.516607
263.324506	4229.593279	7.063693	-0.051331	3.519894
263.366299	4237.617657	7.068698	-0.051344	3.523169
263.814703	4245.690585	7.073702	-0.051433	3.526474
263.756476	4253.750922	7.078707	-0.051427	3.529755
264.170658	4261.735987	7.083712	-0.051509	3.533017
264.794229	4269.747756	7.088717	-0.051631	3.536293
264.751841	4277.781022	7.093722	-0.051628	3.539554
265.460668	4285.776100	7.098726	-0.051765	3.542820
265.538585	4293.861301	7.103731	-0.051785	3.546100
265.652405	4301.875689	7.108736	-0.051811	3.549349
266.253765	4309.923493	7.113741	-0.051928	3.552623
266.352098	4317.976431	7.118746	-0.051952	3.555881
266.641116	4325.943405	7.123750	-0.052011	3.559108
266.625848	4333.967940	7.128755	-0.052013	3.562345
266.734805	4342.032209	7.133760	-0.052039	3.565599
267.149953	4350.003226	7.138765	-0.052121	3.568822
267.360541	4358.065363	7.143770	-0.052166	3.572072
267.730601	4366.074017	7.148774	-0.052240	3.575303
268.568016	4373.977306	7.153779	-0.052401	3.578502
268.441010	4382.122035	7.158784	-0.052382	3.581767
268.776500	4390.075280	7.163789	-0.052450	3.584965
268.781972	4398.177291	7.168794	-0.052456	3.588210
269.425671	4406.216691	7.173798	-0.052581	3.591447
269.718741	4414.141141	7.178803	-0.052641	3.594624
270.039418	4422.164535	7.183808	-0.052706	3.597838
270.211537	4430.259404	7.188813	-0.052743	3.601074
270.200875	4438.277915	7.193818	-0.052746	3.604271
270.181565	4446.364551	7.198822	-0.052748	3.607492
270.540135	4454.332746	7.203827	-0.052820	3.610674
270.912886	4462.380937	7.208832	-0.052894	3.613885
270.802319	4470.455036	7.213837	-0.052879	3.617090
271.394303	4478.374453	7.218842	-0.052994	3.620250
271.723915	4486.434985	7.223846	-0.053061	3.623457
272.102203	4494.428368	7.228851	-0.053137	3.626635
272.312309	4502.485987	7.233856	-0.053181	3.629831
272.661133	4510.544035	7.238861	-0.053251	3.633028
272.643858	4518.573054	7.243866	-0.053253	3.636201
272.863593	4526.574013	7.248870	-0.053299	3.639366
273.228473	4534.543233	7.253875	-0.053372	3.642520
273.217328	4542.602425	7.258880	-0.053375	3.645696
273.947782	4550.586129	7.263885	-0.053516	3.648861
273.970284	4558.657924	7.268890	-0.053526	3.652038
274.590923	4566.661383	7.273894	-0.053647	3.655201
274.653158	4574.676188	7.278899	-0.053663	3.658351
274.823089	4582.737369	7.283904	-0.053700	3.661519
274.905368	4590.766316	7.288909	-0.053721	3.664670
275.185072	4598.766978	7.293914	-0.053778	3.667811
275.154546	4606.884692	7.298918	-0.053778	3.670988
276.009358	4614.735046	7.303923	-0.053942	3.674081
276.126440	4622.843045	7.308928	-0.053969	3.677253
276.100946	4630.899893	7.313933	-0.053969	3.680398
276.310589	4638.865053	7.318938	-0.054013	3.683510
277.004926	4646.883288	7.323942	-0.054148	3.686654
277.165708	4654.916143	7.328947	-0.054183	3.689786
277.470409	4662.960580	7.333952	-0.054245	3.692924
277.315374	4671.089728	7.338957	-0.054221	3.696080
277.711760	4679.001979	7.343962	-0.054300	3.699164
278.060970	4687.054569	7.348966	-0.054370	3.702298
278.652247	4694.944050	7.353971	-0.054486	3.705372
279.068233	4703.057659	7.358976	-0.054568	3.708526
279.036283	4711.177596	7.363981	-0.054568	3.711669
279.067594	4719.187948	7.368986	-0.054579	3.714768
279.174158	4727.239621	7.373990	-0.054604	3.717882
279.514186	4735.198533	7.378995	-0.054672	3.720964
279.815694	4743.144881	7.384000	-0.054733	3.724037
280.105548	4751.216998	7.389005	-0.054793	3.727156
280.168858	4759.291401	7.394010	-0.054810	3.730267
280.853500	4767.219967	7.399014	-0.054942	3.733335
280.977444	4775.283693	7.404019	-0.054971	3.736439
281.218142	4783.298634	7.409024	-0.055021	3.739524
280.995154	4791.426012	7.414029	-0.054984	3.742638
281.146946	4799.392542	7.419034	-0.055018	3.745698
281.974101	4807.360483	7.424038	-0.055177	3.748772
282.291737	4815.421877	7.429043	-0.055241	3.751866
282.743115	4823.423555	7.434048	-0.055330	3.754938
283.296199	4831.409164	7.439053	-0.055439	3.758005
283.537948	4839.467957	7.444058	-0.055489	3.761089
284.047979	4847.433811	7.449062	-0.055589	3.764141
284.490823	4855.478593	7.454067	-0.055677	3.767219
285.033337	4863.497646	7.459072	-0.055783	3.770287
285.146846	4871.563552	7.464077	-0.055809	3.773361
285.233460	4879.604110	7.469082	-0.055830	3.776421
285.804309	4887.574169	7.474086	-0.055942	3.779464
285.715272	4895.664344	7.479091	-0.055930	3.782534
286.342126	4903.591542	7.484096	-0.056052	3.785557
286.482373	4911.697960	7.489101	-0.056084	3.788634
286.865051	4919.716946	7.494106	-0.056160	3.791680
287.373723	4927.711713	7.499110	-0.056260	3.794718
287.375850	4935.759006	7.504115	-0.056266	3.797762
288.019109	4943.759571	7.509120	-0.056391	3.800800
288.354741	4951.754118	7.514125	-0.056458	3.803827
288.586371	4959.732521	7.519130	-0.056506	3.806842
288.949215	4967.841978	7.524134	-0.056579	3.809908
289.344835	4975.845884	7.529139	-0.056658	3.812932
289.262326	4983.927366	7.534144	-0.056648	3.815972
289.952158	4991.847772	7.539149	-0.056782	3.818966
290.450933	4999.863397	7.544154	-0.056880	3.821989
290.799598	5007.936947	7.549158	-0.056950	3.825029
290.719124	5015.998400	7.554163	-0.056940	3.828051
290.747979	5024.073899	7.559168	-0.056951	3.831079
291.580595	5031.985903	7.564173	-0.057111	3.834062
292.032098	5040.004410	7.569178	-0.057200	3.837073
291.832634	5048.125128	7.574182	-0.057168	3.840105
292.439216	5056.020481	7.579187	-0.057286	3.843069
292.584499	5064.110436	7.584192	-0.057318	3.846093
292.828815	5072.146682	7.589197	-0.057369	3.849097
293.735813	5080.079859	7.594202	-0.057543	3.852074
293.929199	5088.176326	7.599206	-0.057584	3.855094
293.965207	5096.184213	7.604211	-0.057596	3.858076
294.483253	5104.217799	7.609216	-0.057698	3.861075
294.554842	5112.239586	7.614221	-0.057716	3.864057
295.228765	5120.229225	7.619226	-0.057847	3.867039
295.140945	5128.308805	7.624230	-0.057836	3.870035
295.327581	5136.454961	7.629235	-0.057876	3.873059
295.294054	5144.494328	7.634240	-0.057875	3.876037
296.022553	5152.340307	7.639245	-0.058016	3.878957
295.967175	5160.379762	7.644250	-0.058010	3.881929
296.121190	5168.437384	7.649254	-0.058044	3.884911
296.296083	5176.375811	7.654259	-0.058082	3.887847
296.210207	5184.483649	7.659264	-0.058071	3.890837
296.766963	5192.415844	7.664269	-0.058180	3.893774
296.758697	5200.475921	7.669274	-0.058184	3.896744
297.456280	5208.427274	7.674278	-0.058319	3.899685
297.769347	5216.454242	7.679283	-0.058382	3.902645
297.858576	5224.488536	7.684288	-0.058404	3.905601
298.320256	5232.541151	7.689293	-0.058495	3.908568
298.167569	5240.620393	7.694298	-0.058472	3.911531
298.456297	5248.610512	7.699302	-0.058531	3.914468
298.886432	5256.603467	7.704307	-0.058616	3.917406
298.937635	5264.633871	7.709312	-0.058631	3.920348
299.505991	5272.590000	7.714317	-0.058742	3.923271
299.392851	5280.680558	7.719322	-0.058726	3.926227
299.840693	5288.697214	7.724326	-0.058815	3.929165
300.479224	5296.723755	7.729331	-0.058939	3.932108
300.646550	5304.728143	7.734336	-0.058975	3.935032
300.721998	5312.807592	7.739341	-0.058994	3.937979
300.793215	5320.816199	7.744346	-0.059013	3.940898
301.484347	5328.754142	7.749350	-0.059146	3.943801
301.482839	5336.836911	7.754355	-0.059151	3.946742
301.869320	5344.847397	7.759360	-0.059229	3.949661
302.330538	5352.897136	7.764365	-0.059320	3.952593
302.420041	5360.928088	7.769370	-0.059342	3.955510
302.831983	5368.916809	7.774374	-0.059423	3.958415
303.268761	5376.928423	7.779379	-0.059510	3.961326
303.526193	5384.899954	7.784384	-0.059563	3.964218
303.892271	5392.968637	7.789389	-0.059636	3.967144
303.934570	5400.990507	7.794394	-0.059649	3.970046
303.843491	5409.065522	7.799398	-0.059638	3.972962
304.075369	5417.100176	7.804403	-0.059686	3.975868
304.626668	5425.019459	7.809408	-0.059794	3.978735
305.129469	5433.044959	7.814413	-0.059893	3.981637
305.218735	5441.001417	7.819418	-0.059914	3.984506
305.762382	5449.115873	7.824422	-0.060021	3.987437
306.006753	5457.159044	7.829427	-0.060072	3.990334
305.959509	5465.210107	7.834432	-0.060068	3.993228
306.219160	5473.213968	7.839437	-0.060121	3.996108
306.237301	5481.177009	7.844442	-0.060130	3.998966
306.318977	5489.295962	7.849446	-0.060150	4.001880
306.808850	5497.182768	7.854451	-0.060247	4.004716
306.932648	5505.273202	7.859456	-0.060275	4.007616
307.757306	5513.228300	7.864461	-0.060434	4.010477
308.030126	5521.272116	7.869466	-0.060490	4.013359
308.132052	5529.369152	7.874470	-0.060514	4.016254
308.567524	5537.274658	7.879475	-0.060600	4.019085
309.086564	5545.286186	7.884480	-0.060702	4.021953
309.060993	5553.372600	7.889485	-0.060702	4.024836
308.971772	5561.463357	7.894490	-0.060691	4.027718
309.433408	5569.460982	7.899494	-0.060782	4.030574
309.700908	5577.512828	7.904499	-0.060837	4.033444
309.744279	5585.557872	7.909504	-0.060850	4.036305
310.135712	5593.500633	7.914509	-0.060928	4.039134
310.591376	5601.490217	7.919514	-0.061018	4.041979
311.111842	5609.438717	7.924518	-0.061120	4.044807
311.334988	5617.490827	7.929523	-0.061167	4.047666
311.723291	5625.504376	7.934528	-0.061245	4.050512
312.168147	5633.528286	7.939533	-0.061333	4.053360
311.832067	5641.624201	7.944538	-0.061275	4.056220
312.288968	5649.597303	7.949542	-0.061366	4.059046
312.633127	5657.648256	7.954547	-0.061435	4.061896
312.735366	5665.663343	7.959552	-0.061459	4.064728
312.948134	5673.738591	7.964557	-0.061504	4.067580
313.077048	5681.722241	7.969562	-0.061533	4.070397
313.361887	5689.782798	7.974566	-0.061591	4.073242
313.470919	5697.758164	7.979571	-0.061617	4.076051
313.592398	5705.762522	7.984576	-0.061645	4.078870
314.117328	5713.813149	7.989581	-0.061748	4.081708
314.201619	5721.776159	7.994586	-0.061768	4.084507
314.492215	5729.868561	7.999590	-0.061828	4.087353
314.646830	5737.837109	8.004595	-0.061862	4.090151
314.807735	5745.894650	8.009600	-0.061897	4.092979
315.218541	5753.901167	8.014605	-0.061978	4.095790
315.920489	5761.885341	8.019610	-0.062114	4.098596
316.386319	5769.919758	8.024614	-0.062206	4.101414
316.825368	5777.828802	8.029619	-0.062293	4.104186
317.184843	5785.935198	8.034624	-0.062365	4.107023
317.145268	5794.010678	8.039629	-0.062363	4.109842
317.136349	5802.040343	8.044634	-0.062367	4.112644
317.581528	5810.024213	8.049638	-0.062455	4.115434
317.557693	5818.086108	8.054643	-0.062455	4.118243
317.838194	5826.046401	8.059648	-0.062513	4.121019
318.349502	5834.006692	8.064653	-0.062613	4.123796
318.752037	5842.033408	8.069658	-0.062693	4.126593
318.818010	5850.087843	8.074662	-0.062711	4.129392
318.951540	5858.107389	8.079667	-0.062741	4.132179
319.416521	5866.092630	8.084672	-0.062833	4.134956
319.791002	5874.170665	8.089677	-0.062908	4.137763
319.570602	5882.202260	8.094682	-0.062872	4.140543
320.105918	5890.167181	8.099686	-0.062977	4.143309
320.692949	5898.206989	8.104691	-0.063091	4.146099
321.014583	5906.196520	8.109696	-0.063156	4.148866
320.970319	5914.279305	8.114701	-0.063153	4.151659
321.385307	5922.236506	8.119706	-0.063235	4.154413
321.384121	5930.339432	8.124710	-0.063240	4.157209
321.543109	5938.293432	8.129715	-0.063275	4.159955
321.968293	5946.286503	8.134720	-0.063360	4.162715
322.489518	5954.265246	8.139725	-0.063462	4.165470
322.324979	5962.385021	8.144730	-0.063436	4.168263
322.768125	5970.411119	8.149734	-0.063524	4.171030
322.782784	5978.418115	8.154739	-0.063532	4.173782
323.333952	5986.442201	8.159744	-0.063640	4.176546
323.405167	5994.466103	8.164749	-0.063658	4.179301
323.708808	6002.454375	8.169754	-0.063720	4.182045
323.823946	6010.496535	8.174758	-0.063747	4.184804
323.928361	6018.533492	8.179763	-0.063771	4.187559
324.128177	6026.536912	8.184768	-0.063814	4.190301
324.909775	6034.563952	8.189773	-0.063964	4.193057
324.867620	6042.650403	8.194778	-0.063962	4.195822
325.287619	6050.613102	8.199782	-0.064045	4.198548
325.439588	6058.648767	8.204787	-0.064079	4.201293
325.952139	6066.545832	8.209792	-0.064179	4.203994
326.213565	6074.648910	8.214797	-0.064233	4.206761
326.531339	6082.596114	8.219802	-0.064297	4.209473
326.557634	6090.744370	8.224806	-0.064307	4.212248
326.581396	6098.718259	8.229811	-0.064317	4.214962
326.942068	6106.767085	8.234816	-0.064389	4.217704
327.355756	6114.735974	8.239821	-0.064472	4.220418
327.559328	6122.714198	8.244826	-0.064515	4.223130
327.987298	6130.734594	8.249830	-0.064599	4.225857
328.235480	6138.826851	8.254835	-0.064651	4.228605
328.770718	6146.836155	8.259840	-0.064756	4.231326
329.240575	6154.768101	8.264845	-0.064848	4.234019
329.345337	6162.832952	8.269850	-0.064873	4.236751
330.040493	6170.811762	8.274854	-0.065008	4.239458
330.085795	6178.836388	8.279859	-0.065021	4.242172
330.294139	6186.865788	8.284864	-0.065065	4.244887
330.735410	6194.910877	8.289869	-0.065153	4.247609
330.827017	6202.924734	8.294874	-0.065175	4.250314
330.965872	6210.949725	8.299878	-0.065206	4.253022
330.789774	6219.041217	8.304883	-0.065178	4.255748
331.137538	6227.005419	8.309888	-0.065248	4.258434
331.243002	6235.071954	8.314893	-0.065273	4.261150
331.688603	6243.017653	8.319898	-0.065361	4.263828
332.372630	6251.009882	8.324902	-0.065494	4.266521
332.329773	6259.049897	8.329907	-0.065491	4.269222
332.544687	6267.066179	8.334912	-0.065536	4.271916
333.059983	6275.099502	8.339917	-0.065637	4.274616
332.988805	6283.124976	8.344922	-0.065629	4.277307
333.014988	6291.155532	8.349926	-0.065639	4.279998
333.113634	6299.149035	8.354931	-0.065663	4.282677
333.474648	6307.107633	8.359936	-0.065735	4.285344
333.906744	6315.139405	8.364941	-0.065821	4.288034
334.166190	6323.194219	8.369946	-0.065874	4.290729
334.773838	6331.174616	8.374950	-0.065993	4.293401
334.914228	6339.240221	8.379955	-0.066024	4.296095
335.247356	6347.194394	8.384960	-0.066091	4.298751
335.680516	6355.281155	8.389965	-0.066177	4.301452
335.467818	6363.245930	8.394970	-0.066143	4.304104
335.933831	6371.310258	8.399974	-0.066235	4.306793
336.709487	6379.283550	8.404979	-0.066384	4.309454
336.927209	6387.335673	8.409984	-0.066430	4.312134
336.919021	6395.418429	8.414989	-0.066434	4.314820
336.919411	6403.355582	8.419994	-0.066439	4.317457
337.678983	6411.335795	8.424998	-0.066585	4.320112
338.026990	6419.357911	8.430003	-0.066655	4.322776
338.481944	6427.325949	8.435008	-0.066745	4.325422
338.784927	6435.427219	8.440013	-0.066807	4.328109
339.464493	6443.361277	8.445018	-0.066939	4.330742
339.626076	6451.457410	8.450022	-0.066974	4.333422
339.525176	6459.576285	8.455027	-0.066960	4.336106
339.875760	6467.483388	8.460032	-0.067031	4.338723
340.031306	6475.590069	8.465037	-0.067065	4.341402
339.945337	6483.462484	8.470042	-0.067054	4.344000
340.063511	6491.617857	8.475046	-0.067081	4.346691
340.335843	6499.554083	8.480051	-0.067137	4.349310
340.630248	6507.583792	8.485056	-0.067197	4.351958
340.789751	6515.637706	8.490061	-0.067232	4.354612
340.922362	6523.620347	8.495066	-0.067262	4.357240
341.514021	6531.572927	8.500070	-0.067377	4.359860
341.430234	6539.652852	8.505075	-0.067367	4.362515
341.932886	6547.593611	8.510080	-0.067465	4.365127
342.116802	6555.633783	8.515085	-0.067505	4.367768
342.257734	6563.694107	8.520090	-0.067536	4.370414
342.750171	6571.709013	8.525094	-0.067633	4.373045
342.568895	6579.775613	8.530099	-0.067605	4.375687
342.673233	6587.744724	8.535104	-0.067629	4.378298
343.129360	6595.774306	8.540109	-0.067719	4.380929
343.229709	6603.782812	8.545114	-0.067743	4.383549
343.311487	6611.775519	8.550118	-0.067764	4.386163
343.753477	6619.772453	8.555123	-0.067851	4.388778
343.969385	6627.848684	8.560128	-0.067897	4.391417
343.944130	6635.897316	8.565133	-0.067897	4.394043
344.073421	6643.922834	8.570138	-0.067926	4.396661
344.667388	6651.859858	8.575143	-0.068042	4.399252
345.021669	6659.908038	8.580147	-0.068113	4.401876
345.507618	6667.845465	8.585152	-0.068209	4.404462
345.662632	6675.969652	8.590157	-0.068243	4.407106
345.687457	6683.938889	8.595162	-0.068253	4.409698
345.969775	6692.038790	8.600167	-0.068310	4.412331
346.277392	6700.021062	8.605171	-0.068373	4.414926
346.547480	6708.081965	8.610176	-0.068428	4.417543
346.663327	6716.131261	8.615181	-0.068455	4.420155
346.961097	6724.075229	8.620186	-0.068516	4.422732
347.196988	6732.123356	8.625191	-0.068565	4.425341
347.463120	6740.184494	8.630195	-0.068620	4.427952
347.498939	6748.209074	8.635200	-0.068631	4.430549
347.619311	6756.237924	8.640205	-0.068659	4.433146
348.000767	6764.269120	8.645210	-0.068735	4.435744
348.159972	6772.258571	8.650215	-0.068770	4.438326
348.326171	6780.233284	8.655219	-0.068806	4.440901
348.521680	6788.217067	8.660224	-0.068848	4.443478
348.874934	6796.327033	8.665229	-0.068919	4.446095
349.312320	6804.254543	8.670234	-0.069005	4.448652
349.772656	6812.324130	8.675239	-0.069096	4.451253
350.017469	6820.323338	8.680243	-0.069147	4.453829
350.129137	6828.391423	8.685248	-0.069173	4.456425
350.303146	6836.342888	8.690253	-0.069211	4.458982
350.817577	6844.368823	8.695258	-0.069312	4.461563
350.839665	6852.394123	8.700263	-0.069321	4.464140
351.158922	6860.456799	8.705267	-0.069385	4.466730
351.618351	6868.411314	8.710272	-0.069476	4.469283
352.132165	6876.478921	8.715277	-0.069577	4.471871
352.113281	6884.443707	8.720282	-0.069579	4.474423
352.360396	6892.518675	8.725287	-0.069630	4.477010
352.948185	6900.409430	8.730291	-0.069744	4.479537
352.964239	6908.519406	8.735296	-0.069753	4.482131
352.997256	6916.513700	8.740301	-0.069764	4.484686
353.401593	6924.564539	8.745306	-0.069844	4.487260
353.659500	6932.542775	8.750311	-0.069898	4.489808
353.831015	6940.630467	8.755315	-0.069935	4.492389
354.156093	6948.541808	8.760320	-0.070000	4.494913
354.889634	6956.593941	8.765325	-0.070142	4.497483
354.837454	6964.603363	8.770330	-0.070138	4.500034
354.900919	6972.685629	8.775335	-0.070155	4.502607
355.529259	6980.629685	8.780339	-0.070277	4.505136
355.457386	6988.704149	8.785344	-0.070269	4.507704
355.854440	6996.665034	8.790349	-0.070348	4.510235
355.728705	7004.768937	8.795354	-0.070330	4.512808
355.951834	7012.728122	8.800359	-0.070376	4.515336
356.246757	7020.677334	8.805363	-0.070436	4.517859
356.877623	7028.700567	8.810368	-0.070559	4.520405
357.349603	7036.729186	8.815373	-0.070652	4.522950
357.246214	7044.743522	8.820378	-0.070638	4.525488
357.270555	7052.768987	8.825383	-0.070648	4.528029
357.704996	7060.826698	8.830387	-0.070734	4.530579
358.071373	7068.794937	8.835392	-0.070807	4.533099
358.170705	7076.862085	8.840397	-0.070831	4.535649
358.301246	7084.852459	8.845402	-0.070860	4.538173
358.732077	7092.848701	8.850407	-0.070946	4.540698
358.669383	7100.837903	8.855411	-0.070939	4.543218
358.743691	7108.898737	8.860416	-0.070958	4.545759
359.145434	7116.919855	8.865421	-0.071038	4.548288
359.438262	7124.943486	8.870426	-0.071098	4.550815
359.425383	7132.929397	8.875431	-0.071101	4.553329
359.982057	7140.981978	8.880435	-0.071210	4.555863
360.181915	7148.943533	8.885440	-0.071252	4.558367
360.238145	7157.049706	8.890445	-0.071268	4.560914
360.509582	7164.927263	8.895450	-0.071323	4.563389
360.838051	7173.014781	8.900455	-0.071390	4.565928
361.297199	7181.057311	8.905459	-0.071480	4.568452
361.598198	7189.051685	8.910464	-0.071542	4.570959
362.202723	7197.070648	8.915469	-0.071659	4.573472
362.442289	7205.079472	8.920474	-0.071709	4.575981
362.846583	7213.052939	8.925479	-0.071790	4.578477
363.378350	7221.081135	8.930483	-0.071894	4.580990
363.548196	7229.061942	8.935488	-0.071931	4.583485
363.616246	7237.166623	8.940493	-0.071948	4.586018
363.667961	7245.192903	8.945498	-0.071963	4.588524
364.055969	7253.231013	8.950503	-0.072041	4.591034
364.249530	7261.232518	8.955507	-0.072082	4.593530
364.654282	7269.187461	8.960512	-0.072162	4.596011
365.159089	7277.238654	8.965517	-0.072262	4.598520
365.133040	7285.259445	8.970522	-0.072262	4.601018
365.245725	7293.171705	8.975527	-0.072288	4.603481
365.732075	7301.256570	8.980531	-0.072384	4.605997
365.796997	7309.214893	8.985536	-0.072401	4.608471
366.144312	7317.307272	8.990541	-0.072471	4.610986
365.931004	7325.296282	8.995546	-0.072436	4.613467
366.255542	7333.369511	9.000551	-0.072502	4.615974
366.660205	7341.312175	9.005555	-0.072582	4.618438
366.656500	7349.379062	9.010560	-0.072587	4.620940
366.952562	7357.346887	9.015565	-0.072647	4.623409
367.531552	7365.296350	9.020570	-0.072760	4.625872
367.620483	7373.393400	9.025575	-0.072782	4.628378
367.793480	7381.491720	9.030579	-0.072819	4.630884
368.007643	7389.437914	9.035584	-0.072864	4.633341
368.202833	7397.505649	9.040589	-0.072906	4.635835
368.492096	7405.425060	9.045594	-0.072965	4.638281
369.256248	7413.473810	9.050599	-0.073112	4.640767
369.290231	7421.484118	9.055603	-0.073124	4.643238
369.122085	7429.556520	9.060608	-0.073098	4.645728
369.498349	7437.536818	9.065613	-0.073173	4.648188
369.819458	7445.541773	9.070618	-0.073238	4.650654
369.818795	7453.592644	9.075623	-0.073243	4.653132
370.470545	7461.629780	9.080627	-0.073370	4.655606
370.250758	7469.598884	9.085632	-0.073334	4.658057
370.743684	7477.638670	9.090637	-0.073431	4.660528
370.848570	7485.608360	9.095642	-0.073456	4.662977
371.073178	7493.639373	9.100647	-0.073503	4.665443
371.364342	7501.666679	9.105651	-0.073562	4.667906
371.223742	7509.698706	9.110656	-0.073541	4.670370
371.603400	7517.779622	9.115661	-0.073617	4.672848
371.529709	7525.752009	9.120666	-0.073608	4.675291
371.611882	7533.728875	9.125671	-0.073629	4.677734
372.306429	7541.686876	9.130675	-0.073763	4.680169
372.728231	7549.673116	9.135680	-0.073847	4.682612
372.749100	7557.724914	9.140685	-0.073856	4.685074
372.792963	7565.778987	9.145690	-0.073869	4.687535
372.893951	7573.799667	9.150695	-0.073893	4.689985
373.071679	7581.863710	9.155699	-0.073932	4.692447
373.401373	7589.758608	9.160704	-0.073998	4.694856
373.729021	7597.878867	9.165709	-0.074064	4.697332
373.519878	7605.875452	9.170714	-0.074031	4.699769
373.666942	7613.920615	9.175719	-0.074063	4.702220
374.127108	7621.821637	9.180723	-0.074154	4.704625
374.699114	7629.902854	9.185728	-0.074266	4.707084
374.636145	7637.940400	9.190733	-0.074259	4.709529
374.815316	7645.951435	9.195738	-0.074298	4.711964
374.798528	7653.938982	9.200743	-0.074300	4.714391
375.224421	7662.051218	9.205747	-0.074384	4.716854
375.485355	7669.905649	9.210752	-0.074438	4.719237
375.617336	7678.038270	9.215757	-0.074468	4.721704
375.969482	7685.910772	9.220762	-0.074538	4.724091
375.946011	7694.086023	9.225767	-0.074539	4.726569
376.094721	7702.087242	9.230771	-0.074572	4.728992
376.425435	7710.117523	9.235776	-0.074639	4.731422
377.216851	7718.071516	9.240781	-0.074792	4.733827
376.980240	7726.183958	9.245786	-0.074753	4.736281
377.501603	7734.115734	9.250791	-0.074855	4.738678
377.568754	7742.163201	9.255795	-0.074873	4.741109
377.654450	7750.129132	9.260800	-0.074894	4.743514
377.851799	7758.215882	9.265805	-0.074936	4.745954
377.852550	7766.267044	9.270810	-0.074941	4.748383
378.126675	7774.267549	9.275815	-0.074997	4.750794
378.413831	7782.309645	9.280819	-0.075056	4.753217
379.133911	7790.263159	9.285824	-0.075195	4.755611
379.267890	7798.304124	9.290829	-0.075225	4.758031
379.795233	7806.248896	9.295834	-0.075329	4.760420
380.092683	7814.276810	9.300839	-0.075389	4.762833
380.540578	7822.315491	9.305843	-0.075478	4.765248
380.463446	7830.312980	9.310848	-0.075469	4.767651
380.761499	7838.348224	9.315853	-0.075529	4.770062
380.944492	7846.412551	9.320858	-0.075569	4.772482
380.971159	7854.417029	9.325863	-0.075579	4.774883
381.187429	7862.464974	9.330867	-0.075624	4.777295
381.716316	7870.395243	9.335872	-0.075728	4.779669
382.234082	7878.464060	9.340877	-0.075829	4.782084
382.070043	7886.448482	9.345882	-0.075804	4.784475
382.162081	7894.526269	9.350887	-0.075826	4.786891
382.911675	7902.475550	9.355891	-0.075971	4.789266
383.168325	7910.513355	9.360896	-0.076024	4.791667
383.652816	7918.485788	9.365901	-0.076119	4.794047
383.961628	7926.553408	9.370906	-0.076182	4.796455
384.157833	7934.518178	9.375911	-0.076224	4.798831
384.370098	7942.602340	9.380915	-0.076269	4.801242
384.620387	7950.481621	9.385920	-0.076320	4.803590
384.814693	7958.614638	9.390925	-0.076362	4.806012
384.709229	7966.645283	9.395930	-0.076347	4.808404
385.051694	7974.641600	9.400935	-0.076416	4.810783
385.771565	7982.639599	9.405939	-0.076555	4.813160
385.821473	7990.066935	9.410944	-0.076569	4.815369
386.041227	7994.746633	9.415949	-0.076613	4.816759

386.138493	7997.378372	9.420954	-0.076633	4.817541
386.377103	7998.631821	9.425959	-0.076678	4.817912
386.396921	7998.974606	9.430963	-0.076682	4.818014
386.470392	7999.939107	9.435968	-0.076696	4.818300
387.017181	8000.007428	9.440973	-0.076798	4.818318
386.888063	8000.065576	9.445978	-0.076774	4.818336
387.135037	8000.006911	9.450983	-0.076820	4.818318
387.509678	8000.022474	9.455987	-0.076890	4.818321
387.689291	7999.935579	9.460992	-0.076923	4.818294
387.978512	7999.969955	9.465997	-0.076977	4.818303
388.148541	7999.949130	9.471002	-0.077009	4.818296
388.590629	7999.923574	9.476007	-0.077091	4.818287
388.837751	7999.950028	9.481011	-0.077137	4.818294
388.771221	7999.948075	9.486016	-0.077124	4.818294
388.952667	8000.026182	9.491021	-0.077158	4.818316
388.854242	7999.997527	9.496026	-0.077140	4.818308
388.665917	8000.040164	9.501031	-0.077105	4.818321
388.520501	8000.106499	9.506035	-0.077078	4.818342
388.975811	8000.008618	9.511040	-0.077162	4.818311
389.124307	8000.009570	9.516045	-0.077190	4.818310
389.083406	8000.013217	9.521050	-0.077182	4.818312
389.222984	7999.964661	9.526055	-0.077208	4.818297
389.713793	7999.956580	9.531059	-0.077300	4.818292
389.426876	7999.986325	9.536064	-0.077246	4.818302
389.502259	8000.097678	9.541069	-0.077260	4.818335
389.337782	8000.093350	9.546074	-0.077229	4.818334
389.148970	8000.065574	9.551079	-0.077194	4.818327
389.332114	8000.137402	9.556083	-0.077228	4.818348
389.559245	8000.052199	9.561088	-0.077271	4.818321
389.916776	8000.008690	9.566093	-0.077337	4.818307
389.669760	8000.090466	9.571098	-0.077291	4.818332
389.408385	8000.158386	9.576103	-0.077242	4.818354
389.702391	8000.112968	9.581107	-0.077297	4.818339
389.363149	8000.152513	9.586112	-0.077234	4.818352
389.667965	8000.192360	9.591117	-0.077291	4.818363
389.740579	8000.189136	9.596122	-0.077304	4.818361
389.828110	8000.115705	9.601127	-0.077320	4.818339
390.100140	8000.121482	9.606131	-0.077371	4.818340
390.073456	8000.120067	9.611136	-0.077366	4.818339
389.919240	8000.170521	9.616141	-0.077337	4.818355
389.841160	8000.145293	9.621146	-0.077323	4.818348
390.026938	8000.145700	9.626151	-0.077357	4.818347
390.133852	8000.208093	9.631155	-0.077377	4.818365
390.044894	8000.154343	9.636160	-0.077360	4.818350
390.290214	8000.156607	9.641165	-0.077406	4.818349
390.358215	8000.169083	9.646170	-0.077419	4.818353
390.623335	8000.150598	9.651175	-0.077468	4.818346
391.225406	8000.075721	9.656179	-0.077580	4.818322
391.116599	8000.034312	9.661184	-0.077560	4.818310
390.682360	8000.156641	9.666189	-0.077479	4.818348
390.521255	8000.101915	9.671194	-0.077449	4.818332
390.829265	8000.097671	9.676199	-0.077506	4.818330
390.618715	8000.157872	9.681203	-0.077467	4.818349
390.666484	8000.112276	9.686208	-0.077476	4.818335
390.973360	8000.117475	9.691213	-0.077533	4.818335
390.834652	8000.153427	9.696218	-0.077507	4.818346
391.137498	8000.045077	9.701223	-0.077563	4.818313
390.954357	8000.156091	9.706227	-0.077529	4.818347
390.697498	8000.146307	9.711232	-0.077481	4.818345
391.087208	8000.145271	9.716237	-0.077554	4.818343
390.945728	8000.194847	9.721242	-0.077527	4.818358
391.256124	8000.100261	9.726247	-0.077585	4.818329
391.323039	8000.115875	9.731251	-0.077597	4.818333
391.645537	7999.946840	9.736256	-0.077657	4.818282
391.902708	7999.991301	9.741261	-0.077705	4.818294
391.715752	8000.077042	9.746266	-0.077670	4.818320
391.763317	8000.059818	9.751271	-0.077679	4.818315
392.034268	8000.037209	9.756275	-0.077730	4.818307
391.868253	8000.098013	9.761280	-0.077699	4.818326
391.524860	8000.148008	9.766285	-0.077635	4.818342
391.409446	8000.130680	9.771290	-0.077613	4.818337
391.460527	8000.089332	9.776295	-0.077623	4.818325
391.554063	8000.111612	9.781299	-0.077640	4.818331
391.962846	8000.005747	9.786304	-0.077716	4.818298
391.900125	8000.045879	9.791309	-0.077704	4.818310
391.800625	8000.047682	9.796314	-0.077686	4.818311
392.227174	8000.015620	9.801319	-0.077765	4.818300
392.162183	8000.075689	9.806323	-0.077753	4.818318
391.966678	8000.081447	9.811328	-0.077717	4.818320
392.030206	8000.091761	9.816333	-0.077728	4.818323
392.002362	8000.099788	9.821338	-0.077723	4.818326
392.271467	8000.065595	9.826343	-0.077773	4.818315
392.301806	8000.119599	9.831347	-0.077779	4.818330
391.992256	8000.036588	9.836352	-0.077721	4.818307
392.172585	8000.096825	9.841357	-0.077755	4.818324
392.138685	8000.083752	9.846362	-0.077748	4.818320
391.905947	8000.105820	9.851367	-0.077705	4.818328
392.057305	8000.090000	9.856371	-0.077733	4.818323
392.381577	8000.042892	9.861376	-0.077793	4.818307
392.529516	7999.993397	9.866381	-0.077821	4.818292
392.027806	8000.095896	9.871386	-0.077727	4.818325
392.449502	8000.005969	9.876391	-0.077806	4.818296
392.453335	8000.080632	9.881395	-0.077807	4.818318
392.297533	8000.022822	9.886400	-0.077777	4.818302
392.781769	7999.991541	9.891405	-0.077868	4.818290
392.398216	8000.040992	9.896410	-0.077796	4.818307
392.531225	8000.020721	9.901415	-0.077821	4.818300
392.744875	8000.059341	9.906419	-0.077861	4.818311
392.816812	7999.995155	9.911424	-0.077874	4.818291
392.474519	8000.090354	9.916429	-0.077810	4.818321
392.192574	8000.144334	9.921434	-0.077758	4.818338
392.430747	8000.100264	9.926439	-0.077802	4.818324
392.348802	8000.153799	9.931443	-0.077787	4.818340
392.417574	8000.058043	9.936448	-0.077799	4.818312
392.228263	8000.127989	9.941453	-0.077764	4.818333
392.337952	8000.160998	9.946458	-0.077785	4.818343
392.545108	8000.123865	9.951463	-0.077823	4.818331
392.213591	8000.179275	9.956467	-0.077761	4.818349
392.157540	8000.117561	9.961472	-0.077751	4.818330
392.634753	8000.176564	9.966477	-0.077840	4.818346
392.716022	8000.162949	9.971482	-0.077855	4.818342
392.549931	8000.200631	9.976487	-0.077824	4.818354
392.626385	8000.148066	9.981491	-0.077838	4.818338
392.680414	8000.087841	9.986496	-0.077848	4.818320
392.736605	8000.121177	9.991501	-0.077858	4.818329
392.787797	8000.115562	9.996506	-0.077868	4.818327
393.129832	8000.038218	10.001511	-0.077931	4.818303
393.546223	8000.041752	10.006515	-0.078009	4.818302
393.206493	8000.063421	10.011520	-0.077946	4.818310
393.104986	8000.121946	10.016525	-0.077927	4.818328
393.120352	8000.120049	10.021530	-0.077930	4.818327
393.027679	8000.079906	10.026535	-0.077912	4.818316
393.259302	8000.140841	10.031539	-0.077955	4.818333
393.744012	7999.966643	10.036544	-0.078045	4.818279
393.554050	8000.042886	10.041549	-0.078010	4.818303
393.463426	8000.105763	10.046554	-0.077993	4.818322
393.965705	8000.024285	10.051559	-0.078087	4.818295
393.826279	8000.070736	10.056563	-0.078061	4.818310
393.776005	7999.982823	10.061568	-0.078051	4.818284
394.060101	7999.999280	10.066573	-0.078104	4.818288
394.142660	8000.014057	10.071578	-0.078119	4.818292
393.308057	8000.121504	10.076583	-0.077964	4.818327
393.775434	8000.034299	10.081587	-0.078051	4.818299
393.054878	8000.132782	10.086592	-0.077917	4.818331
393.313131	8000.115258	10.091597	-0.077965	4.818325
393.498606	8000.059965	10.096602	-0.077999	4.818308
393.304768	8000.098323	10.101607	-0.077963	4.818320
393.422955	8000.106226	10.106611	-0.077985	4.818322
393.294103	8000.065593	10.111616	-0.077961	4.818310
393.041068	8000.168306	10.116621	-0.077914	4.818342
392.890691	8000.207253	10.121626	-0.077886	4.818354
392.671986	8000.134926	10.126631	-0.077845	4.818334
392.825189	8000.190595	10.131635	-0.077874	4.818349
393.052725	8000.191572	10.136640	-0.077916	4.818349
392.912352	8000.231704	10.141645	-0.077890	4.818361
392.819506	8000.233596	10.146650	-0.077872	4.818362
392.963707	8000.196662	10.151655	-0.077899	4.818351
393.017936	8000.214208	10.156659	-0.077909	4.818356
393.077775	8000.192945	10.161664	-0.077920	4.818349
393.344142	8000.110374	10.166669	-0.077970	4.818324
393.350904	8000.178773	10.171674	-0.077971	4.818344
393.451337	8000.064527	10.176679	-0.077990	4.818310
393.473756	8000.173074	10.181683	-0.077994	4.818342
393.185814	8000.189138	10.186688	-0.077940	4.818348
393.331355	8000.218431	10.191693	-0.077967	4.818356
392.919408	8000.259088	10.196698	-0.077891	4.818369
393.137178	8000.221048	10.201703	-0.077931	4.818357
393.251054	8000.255167	10.206707	-0.077952	4.818367
393.143809	8000.164381	10.211712	-0.077932	4.818340
393.269041	8000.210213	10.216717	-0.077956	4.818354
393.593526	8000.169416	10.221722	-0.078016	4.818340
393.294106	8000.260992	10.226727	-0.077960	4.818369
393.169089	8000.247734	10.231731	-0.077937	4.818365
393.545849	8000.099398	10.236736	-0.078007	4.818320
393.850456	8000.086706	10.241741	-0.078063	4.818315
393.734093	8000.100890	10.246746	-0.078042	4.818319
393.453168	8000.178004	10.251751	-0.077989	4.818343
393.495899	8000.194343	10.256755	-0.077997	4.818348
393.821265	8000.044259	10.261760	-0.078058	4.818302
393.595567	8000.128427	10.266765	-0.078016	4.818328
393.638164	8000.145816	10.271770	-0.078024	4.818333
393.757546	8000.119054	10.276775	-0.078046	4.818325
393.803869	8000.112322	10.281779	-0.078054	4.818322
393.940434	8000.049010	10.286784	-0.078080	4.818303
393.723326	8000.149058	10.291789	-0.078039	4.818334
393.821330	8000.181911	10.296794	-0.078058	4.818343
393.784959	8000.156192	10.301799	-0.078051	4.818335
393.893108	8000.224916	10.306803	-0.078071	4.818355
393.583123	8000.236476	10.311808	-0.078013	4.818360
393.668058	8000.193484	10.316813	-0.078029	4.818347
393.725421	8000.183748	10.321818	-0.078040	4.818344
393.986189	8000.046451	10.326823	-0.078088	4.818302
393.941512	8000.111001	10.331827	-0.078080	4.818321
394.147473	8000.108534	10.336832	-0.078118	4.818320
394.202498	8000.055678	10.341837	-0.078128	4.818304
394.379550	8000.019188	10.346842	-0.078161	4.818292
394.173069	8000.099412	10.351847	-0.078123	4.818317
393.961054	8000.196377	10.356851	-0.078083	4.818347
393.870012	8000.146796	10.361856	-0.078066	4.818332
393.916483	8000.105384	10.366861	-0.078075	4.818320
393.848221	8000.179074	10.371866	-0.078062	4.818342
394.392800	8000.025654	10.376871	-0.078163	4.818294
394.049177	8000.104019	10.381875	-0.078099	4.818319
393.999938	8000.109655	10.386880	-0.078090	4.818321
394.057805	8000.202920	10.391885	-0.078101	4.818348
394.092762	8000.120364	10.396890	-0.078107	4.818324
394.017986	8000.094125	10.401895	-0.078093	4.818316
393.900439	8000.154535	10.406899	-0.078071	4.818334
393.715382	8000.079509	10.411904	-0.078037	4.818313
393.723622	8000.144776	10.416909	-0.078038	4.818332
394.163253	8000.072959	10.421914	-0.078120	4.818309
394.144034	8000.049575	10.426919	-0.078116	4.818302
394.272418	8000.055515	10.431923	-0.078140	4.818304
394.118142	8000.033453	10.436928	-0.078112	4.818298
394.318712	8000.074002	10.441933	-0.078149	4.818309
393.864246	8000.144560	10.446938	-0.078064	4.818332
393.806058	8000.146921	10.451943	-0.078053	4.818333
394.204770	8000.089263	10.456947	-0.078127	4.818314
394.290634	8000.057844	10.461952	-0.078143	4.818304
394.188340	8000.101645	10.466957	-0.078124	4.818318
395.011709	8000.019265	10.471962	-0.078278	4.818290
394.265776	8000.070109	10.476967	-0.078139	4.818308
394.647667	8000.095249	10.481971	-0.078210	4.818314
394.498133	8000.080607	10.486976	-0.078182	4.818310
394.459799	8000.084288	10.491981	-0.078175	4.818311
394.589948	8000.057673	10.496986	-0.078199	4.818303
394.252625	8000.042589	10.501991	-0.078136	4.818300
394.321217	8000.178038	10.506995	-0.078149	4.818340
394.164005	8000.119152	10.512000	-0.078119	4.818323
394.400820	8000.088728	10.517005	-0.078163	4.818313
394.251672	8000.150811	10.522010	-0.078136	4.818332
394.022837	8000.098312	10.527015	-0.078093	4.818317
394.093250	8000.147607	10.532019	-0.078106	4.818332
394.171066	8000.087703	10.537024	-0.078120	4.818314
393.981120	8000.114552	10.542029	-0.078085	4.818322
394.150696	8000.155732	10.547034	-0.078117	4.818334
394.093503	8000.203298	10.552039	-0.078106	4.818348
394.273883	8000.188924	10.557043	-0.078140	4.818343
394.513251	8000.102833	10.562048	-0.078184	4.818317
394.292163	8000.164993	10.567053	-0.078143	4.818336
394.708511	8000.016141	10.572058	-0.078220	4.818290
395.205560	7999.969275	10.577063	-0.078313	4.818274
394.873203	8000.069864	10.582067	-0.078251	4.818305
394.699004	8000.073805	10.587072	-0.078218	4.818307
395.260738	8000.041479	10.592077	-0.078323	4.818295
394.936732	8000.106448	10.597082	-0.078263	4.818316
394.716671	8000.084545	10.602087	-0.078221	4.818310
394.796647	8000.148683	10.607091	-0.078236	4.818329
394.673532	8000.093412	10.612096	-0.078213	4.818313
394.693075	8000.110489	10.617101	-0.078217	4.818318
394.760651	8000.147135	10.622106	-0.078230	4.818329
394.776283	8000.098999	10.627111	-0.078232	4.818315
394.592505	8000.190041	10.632115	-0.078198	4.818342
394.832457	8000.049307	10.637120	-0.078243	4.818300
394.977116	8000.031296	10.642125	-0.078270	4.818294
394.885190	8000.084697	10.647130	-0.078252	4.818310
394.699142	8000.097937	10.652135	-0.078218	4.818315
394.570397	8000.139278	10.657139	-0.078194	4.818327
394.354566	8000.136349	10.662144	-0.078154	4.818327
394.646027	8000.069882	10.667149	-0.078208	4.818306
395.035615	8000.028916	10.672154	-0.078280	4.818293
395.081965	8000.029541	10.677159	-0.078289	4.818293
395.003890	8000.025327	10.682163	-0.078274	4.818292
394.650636	8000.018434	10.687168	-0.078208	4.818291
394.660086	8000.090024	10.692173	-0.078210	4.818312
394.601544	8000.044036	10.697178	-0.078199	4.818299
394.302362	8000.112494	10.702183	-0.078143	4.818320
394.629175	8000.125328	10.707187	-0.078204	4.818323
394.885036	8000.049970	10.712192	-0.078252	4.818300
395.016798	8000.086435	10.717197	-0.078276	4.818310
394.482087	8000.171669	10.722202	-0.078177	4.818337
394.582607	8000.137295	10.727207	-0.078195	4.818327
394.700626	8000.177778	10.732211	-0.078217	4.818338
394.648169	8000.129770	10.737216	-0.078208	4.818324
395.246552	8000.023322	10.742221	-0.078319	4.818290
395.022676	8000.095954	10.747226	-0.078277	4.818313
394.695537	8000.090465	10.752231	-0.078216	4.818312
395.002231	8000.050478	10.757235	-0.078273	4.818299
394.757057	8000.070273	10.762240	-0.078228	4.818306
394.772230	8000.086240	10.767245	-0.078230	4.818311
395.054995	8000.116344	10.772250	-0.078283	4.818319
394.616650	8000.169253	10.777255	-0.078201	4.818336
394.950769	8000.212665	10.782259	-0.078264	4.818348
394.924446	8000.108258	10.787264	-0.078259	4.818317
394.994260	8000.103947	10.792269	-0.078271	4.818315
395.538440	8000.041956	10.797274	-0.078373	4.818295
395.478157	7999.984383	10.802279	-0.078361	4.818278
395.190758	8000.137079	10.807283	-0.078308	4.818324
395.177902	8000.076996	10.812288	-0.078305	4.818306
395.123220	8000.058385	10.817293	-0.078295	4.818301
395.021770	8000.063312	10.822298	-0.078276	4.818303
395.256663	7999.998179	10.827303	-0.078320	4.818283
395.170206	8000.075827	10.832307	-0.078304	4.818306
394.963453	8000.046747	10.837312	-0.078265	4.818298
395.388071	8000.005206	10.842317	-0.078344	4.818284
395.667511	8000.012144	10.847322	-0.078396	4.818285
395.886065	7999.952045	10.852327	-0.078437	4.818266
395.445587	8000.000721	10.857331	-0.078355	4.818283
395.393029	8000.086185	10.862336	-0.078345	4.818308
395.380728	8000.039772	10.867341	-0.078343	4.818295
395.000578	8000.150223	10.872346	-0.078272	4.818329
395.148033	8000.021897	10.877351	-0.078299	4.818290
395.444872	8000.087926	10.882355	-0.078355	4.818309
395.485726	8000.004398	10.887360	-0.078362	4.818284
395.398574	8000.048405	10.892365	-0.078346	4.818297
395.362264	8000.095204	10.897370	-0.078339	4.818311
395.526546	8000.046981	10.902375	-0.078370	4.818296
395.708265	8000.016861	10.907379	-0.078403	4.818286
395.268383	8000.089717	10.912384	-0.078321	4.818310
395.687368	8000.040744	10.917389	-0.078399	4.818294
395.235373	8000.123946	10.922394	-0.078315	4.818320
395.079847	8000.107120	10.927399	-0.078286	4.818316
395.346340	8000.197962	10.932403	-0.078336	4.818342
395.380315	8000.051281	10.937408	-0.078342	4.818298
395.445284	8000.054261	10.942413	-0.078354	4.818299
395.560241	8000.131487	10.947418	-0.078375	4.818321
395.514163	8000.064647	10.952423	-0.078367	4.818301
395.679752	8000.077399	10.957427	-0.078398	4.818305
395.007824	8000.167077	10.962432	-0.078272	4.818334
395.124211	8000.180213	10.967437	-0.078294	4.818337
395.320879	8000.168162	10.972442	-0.078331	4.818333
395.040885	8000.128629	10.977447	-0.078278	4.818322
395.424773	8000.122270	10.982451	-0.078350	4.818319
395.426093	8000.121234	10.987456	-0.078350	4.818319
395.392827	8000.129187	10.992461	-0.078344	4.818321
395.279817	8000.210680	10.997466	-0.078323	4.818346
395.141860	8000.092147	11.002471	-0.078297	4.818311
395.315981	8000.107116	11.007475	-0.078329	4.818315
395.199220	8000.107631	11.012480	-0.078308	4.818315
395.287553	8000.171885	11.017485	-0.078324	4.818334
395.334287	8000.152546	11.022490	-0.078333	4.818328
395.347755	8000.086514	11.027495	-0.078335	4.818309
395.647416	8000.154684	11.032499	-0.078391	4.818328
395.364668	8000.116164	11.037504	-0.078338	4.818317
395.340134	8000.091655	11.042509	-0.078334	4.818310
395.618847	8000.067055	11.047514	-0.078385	4.818302
395.470995	8000.140718	11.052519	-0.078358	4.818324
395.271321	8000.154823	11.057523	-0.078321	4.818329
395.082800	8000.171181	11.062528	-0.078286	4.818335
395.240733	8000.208001	11.067533	-0.078315	4.818345
395.137046	8000.178216	11.072538	-0.078296	4.818337
395.124641	8000.079252	11.077543	-0.078293	4.818307
395.392863	8000.162760	11.082547	-0.078343	4.818331
395.139948	8000.163531	11.087552	-0.078296	4.818332
394.796654	8000.215627	11.092557	-0.078232	4.818349
395.043386	8000.173776	11.097562	-0.078278	4.818336
395.305370	8000.085890	11.102567	-0.078327	4.818309
395.483300	8000.097758	11.107571	-0.078360	4.818311
395.882199	8000.031696	11.112576	-0.078434	4.818290
395.526936	8000.089935	11.117581	-0.078368	4.818309
395.792800	8000.120863	11.122586	-0.078417	4.818317
395.427219	8000.050741	11.127591	-0.078349	4.818298
395.858634	8000.088117	11.132595	-0.078429	4.818307
395.766915	8000.044830	11.137600	-0.078412	4.818295
395.925383	8000.011242	11.142605	-0.078442	4.818284
395.602041	8000.163452	11.147610	-0.078381	4.818330
395.843319	8000.033245	11.152615	-0.078426	4.818291
395.926437	8000.075357	11.157619	-0.078442	4.818303
395.864962	8000.051398	11.162624	-0.078430	4.818296
395.731787	8000.055895	11.167629	-0.078405	4.818298
396.173660	7999.987263	11.172634	-0.078488	4.818276
395.955167	7999.966430	11.177639	-0.078447	4.818270
395.725421	8000.136725	11.182643	-0.078404	4.818322
395.505306	8000.137941	11.187648	-0.078363	4.818323
395.393855	8000.133273	11.192653	-0.078342	4.818322
395.349618	8000.169455	11.197658	-0.078334	4.818333
395.622186	8000.096425	11.202663	-0.078385	4.818310
395.399576	8000.189043	11.207667	-0.078343	4.818339
395.662912	8000.119042	11.212672	-0.078392	4.818317
396.142004	8000.015181	11.217677	-0.078481	4.818284
396.105711	8000.027298	11.222682	-0.078474	4.818288
395.949403	8000.024124	11.227687	-0.078445	4.818288
395.938131	8000.035529	11.232691	-0.078443	4.818291
396.247891	8000.017655	11.237696	-0.078501	4.818285
395.995292	8000.025787	11.242701	-0.078454	4.818288
396.425380	7999.970659	11.247706	-0.078534	4.818270
396.472079	7999.991258	11.252711	-0.078542	4.818276
396.899063	7999.962363	11.257715	-0.078622	4.818265
396.584398	7999.955990	11.262720	-0.078563	4.818265
396.488717	7999.982015	11.267725	-0.078545	4.818273
396.917269	7999.961549	11.272730	-0.078625	4.818265
396.432523	7999.985450	11.277735	-0.078535	4.818274
396.369926	8000.035046	11.282739	-0.078523	4.818289
396.382030	7999.992116	11.287744	-0.078525	4.818276
396.029159	8000.062998	11.292749	-0.078460	4.818299
396.119944	8000.137796	11.297754	-0.078477	4.818321
396.426996	8000.017940	11.302759	-0.078534	4.818284
396.362371	8000.025468	11.307763	-0.078522	4.818286
395.939748	8000.070181	11.312768	-0.078443	4.818301
396.329459	8000.009250	11.317773	-0.078515	4.818282
396.710330	8000.018617	11.322778	-0.078586	4.818283
396.172207	8000.000805	11.327783	-0.078486	4.818280
396.650829	8000.031466	11.332787	-0.078575	4.818287
396.668128	8000.001218	11.337792	-0.078578	4.818278
396.275440	8000.033725	11.342797	-0.078505	4.818289
396.076029	8000.122454	11.347802	-0.078468	4.818316
396.212116	8000.083307	11.352807	-0.078493	4.818304
396.526482	8000.044477	11.357811	-0.078552	4.818291
396.444416	8000.027595	11.362816	-0.078536	4.818287
396.558394	8000.070127	11.367821	-0.078557	4.818299
396.664285	8000.050540	11.372826	-0.078577	4.818293
396.441440	8000.023341	11.377831	-0.078536	4.818285
396.407766	8000.042850	11.382835	-0.078529	4.818291
396.456074	7999.993054	11.387840	-0.078538	4.818276
396.507850	7999.992702	11.392845	-0.078548	4.818276
396.090491	8000.082679	11.397850	-0.078470	4.818305
396.227267	7999.988890	11.402855	-0.078495	4.818276
396.592265	8000.027469	11.407859	-0.078563	4.818286
396.584008	8000.015793	11.412864	-0.078562	4.818283
396.423009	8000.020963	11.417869	-0.078532	4.818285
396.598079	8000.019130	11.422874	-0.078564	4.818284
396.692525	7999.983623	11.427879	-0.078582	4.818273
396.652778	8000.024070	11.432883	-0.078574	4.818285
396.641563	8000.041781	11.437888	-0.078572	4.818290
396.795222	8000.027046	11.442893	-0.078601	4.818285
396.994348	8000.008724	11.447898	-0.078638	4.818279
397.103374	7999.969210	11.452903	-0.078658	4.818267
396.583700	8000.054646	11.457907	-0.078561	4.818294
396.732272	8000.011465	11.462912	-0.078589	4.818281
396.511111	8000.049451	11.467917	-0.078548	4.818293
396.689868	8000.049771	11.472922	-0.078581	4.818292
396.717073	8000.011249	11.477927	-0.078586	4.818281
396.668621	8000.046323	11.482931	-0.078577	4.818291
396.294075	8000.120064	11.487936	-0.078507	4.818315
396.352025	8000.099827	11.492941	-0.078518	4.818309
396.039768	8000.243780	11.497946	-0.078460	4.818353
396.243316	8000.144590	11.502951	-0.078498	4.818322
395.937204	8000.217158	11.507955	-0.078441	4.818345
396.031760	8000.164836	11.512960	-0.078458	4.818329
396.002739	8000.187561	11.517965	-0.078453	4.818336
396.168256	8000.205568	11.522970	-0.078484	4.818341
395.947240	8000.112180	11.527975	-0.078442	4.818314
396.192214	8000.131265	11.532979	-0.078488	4.818319
396.323825	8000.091007	11.537984	-0.078512	4.818306
396.064717	8000.162110	11.542989	-0.078464	4.818328
396.374836	8000.131630	11.547994	-0.078522	4.818318
396.275198	8000.090337	11.552999	-0.078503	4.818306
396.669888	8000.058903	11.558003	-0.078577	4.818295
396.169241	8000.149852	11.563008	-0.078483	4.818324
396.477756	8000.016351	11.568013	-0.078541	4.818283
396.529308	8000.087465	11.573018	-0.078550	4.818304
396.478195	8000.052085	11.578023	-0.078541	4.818294
395.853659	8000.157119	11.583027	-0.078424	4.818328
396.113228	8000.115443	11.588032	-0.078473	4.818314
396.166759	8000.100401	11.593037	-0.078483	4.818310
396.370679	8000.142051	11.598042	-0.078521	4.818321
396.843287	8000.004471	11.603047	-0.078608	4.818278
396.671001	8000.075701	11.608051	-0.078576	4.818300
396.703941	8000.067736	11.613056	-0.078582	4.818298
396.549645	8000.028855	11.618061	-0.078554	4.818287
396.502192	8000.115441	11.623066	-0.078545	4.818313
396.685855	7999.993910	11.628071	-0.078579	4.818276
396.673187	8000.059949	11.633075	-0.078576	4.818295
396.754789	8000.033726	11.638080	-0.078592	4.818287
396.630723	8000.040448	11.643085	-0.078568	4.818290
396.521632	8000.117791	11.648090	-0.078548	4.818313
396.587677	8000.030399	11.653095	-0.078560	4.818287
396.397587	8000.105591	11.658099	-0.078525	4.818310
396.493307	8000.102682	11.663104	-0.078543	4.818309
396.117104	8000.200574	11.668109	-0.078473	4.818339
396.503126	8000.100707	11.673114	-0.078544	4.818308
396.470421	8000.045608	11.678119	-0.078538	4.818292
396.217476	8000.099979	11.683123	-0.078491	4.818309
396.368650	8000.129352	11.688128	-0.078519	4.818317
396.481932	8000.056264	11.693133	-0.078540	4.818295
396.353966	8000.099718	11.698138	-0.078516	4.818309
396.800417	7999.995415	11.703143	-0.078599	4.818276
396.676598	8000.058895	11.708147	-0.078576	4.818295
397.052523	8000.014594	11.713152	-0.078646	4.818280
396.437437	8000.069307	11.718157	-0.078532	4.818299
396.735319	8000.114334	11.723162	-0.078587	4.818311
396.722826	8000.040591	11.728167	-0.078585	4.818290
396.570574	8000.083715	11.733171	-0.078556	4.818303
396.623806	8000.071822	11.738176	-0.078566	4.818299
396.744798	8000.071358	11.743181	-0.078589	4.818299
396.746668	8000.115523	11.748186	-0.078589	4.818312
396.884478	8000.040665	11.753191	-0.078615	4.818289
396.979249	8000.069274	11.758195	-0.078632	4.818297
396.574597	8000.114229	11.763200	-0.078557	4.818312
396.884178	8000.050110	11.768205	-0.078615	4.818292
397.121961	8000.050180	11.773210	-0.078659	4.818291
396.863340	8000.049821	11.778215	-0.078611	4.818292
396.935599	8000.118063	11.783219	-0.078624	4.818312
396.812527	8000.155278	11.788224	-0.078601	4.818323
396.669460	8000.096578	11.793229	-0.078574	4.818306
397.000825	8000.073745	11.798234	-0.078636	4.818298
396.585480	8000.112249	11.803239	-0.078559	4.818311
396.960384	8000.075291	11.808243	-0.078628	4.818299
396.958876	8000.088931	11.813248	-0.078628	4.818303
397.015880	8000.017181	11.818253	-0.078639	4.818281
396.992315	8000.037878	11.823258	-0.078634	4.818288
397.396448	8000.018134	11.828263	-0.078709	4.818280
396.948091	8000.124506	11.833267	-0.078626	4.818314
396.433970	8000.195302	11.838272	-0.078530	4.818337
396.531000	8000.139861	11.843277	-0.078548	4.818320
397.193130	8000.061607	11.848282	-0.078671	4.818294
397.057099	8000.006156	11.853287	-0.078646	4.818278
397.430679	8000.048007	11.858291	-0.078715	4.818289
397.155208	8000.086307	11.863296	-0.078664	4.818301
397.185245	8000.046772	11.868301	-0.078670	4.818290
396.947221	8000.142335	11.873306	-0.078625	4.818319
396.838878	8000.110382	11.878311	-0.078605	4.818310
396.999939	8000.076830	11.883315	-0.078635	4.818299
396.544074	8000.157876	11.888320	-0.078550	4.818325
396.743889	8000.144818	11.893325	-0.078587	4.818320
397.449786	8000.069261	11.898330	-0.078719	4.818295
397.151198	8000.050491	11.903335	-0.078663	4.818291
396.855664	8000.102182	11.908339	-0.078608	4.818307
396.714081	8000.181186	11.913344	-0.078582	4.818331
396.447111	8000.253234	11.918349	-0.078532	4.818354
396.357801	8000.262529	11.923354	-0.078515	4.818357
396.804585	8000.145619	11.928359	-0.078598	4.818320
396.726770	8000.239151	11.933363	-0.078584	4.818349
396.591793	8000.152184	11.938368	-0.078559	4.818323
396.879441	8000.164492	11.943373	-0.078612	4.818326
396.741658	8000.205711	11.948378	-0.078586	4.818339
396.645101	8000.182326	11.953383	-0.078568	4.818332
396.584062	8000.198311	11.958387	-0.078557	4.818337
396.729804	8000.207642	11.963392	-0.078584	4.818339
396.574748	8000.221300	11.968397	-0.078555	4.818344
396.909999	8000.165938	11.973402	-0.078618	4.818326
396.903915	8000.064954	11.978407	-0.078616	4.818296
397.082827	8000.088399	11.983411	-0.078650	4.818302
396.460151	8000.193456	11.988416	-0.078534	4.818336
396.820227	8000.096390	11.993421	-0.078601	4.818306
397.401456	8000.070641	11.998426	-0.078709	4.818296
397.068350	8000.026179	12.003431	-0.078647	4.818284
397.228759	8000.051474	12.008435	-0.078677	4.818291
398.122367	7999.931169	12.013440	-0.078843	4.818251
397.559977	7999.960319	12.018445	-0.078738	4.818262
397.339919	8000.042463	12.023450	-0.078697	4.818288
397.884211	7999.971019	12.028455	-0.078798	4.818264
397.654785	8000.042525	12.033459	-0.078756	4.818286
397.468792	8000.039998	12.038464	-0.078721	4.818286
398.097657	7999.982314	12.043469	-0.078838	4.818267
398.220121	7999.995535	12.048474	-0.078861	4.818270
397.947792	7999.951896	12.053479	-0.078810	4.818258
397.550029	8000.049495	12.058483	-0.078736	4.818289
397.672843	8000.044853	12.063488	-0.078759	4.818287
397.518112	8000.040647	12.068493	-0.078730	4.818286
397.498606	8000.046685	12.073498	-0.078726	4.818288
397.543876	8000.011561	12.078503	-0.078735	4.818278
397.734757	8000.050935	12.083507	-0.078770	4.818289
397.320741	8000.098915	12.088512	-0.078693	4.818305
397.636976	8000.027529	12.093517	-0.078752	4.818282
397.510993	8000.125664	12.098522	-0.078728	4.818312
397.534182	8000.089190	12.103527	-0.078733	4.818301
397.723538	8000.100165	12.108531	-0.078768	4.818303
397.528090	8000.179490	12.113536	-0.078731	4.818328
397.414236	8000.150614	12.118541	-0.078710	4.818320
397.445788	8000.149988	12.123546	-0.078716	4.818319
397.172580	8000.125256	12.128551	-0.078665	4.818313
397.572352	8000.086535	12.133555	-0.078739	4.818300
397.667459	8000.034220	12.138560	-0.078757	4.818284
397.483002	8000.049581	12.143565	-0.078723	4.818289
397.614258	8000.080788	12.148570	-0.078747	4.818298
397.471108	8000.053617	12.153575	-0.078720	4.818290
397.668851	8000.063654	12.158579	-0.078757	4.818293
397.761057	8000.054392	12.163584	-0.078774	4.818290
397.872189	8000.004397	12.168589	-0.078795	4.818274
397.393943	8000.139792	12.173594	-0.078706	4.818316
396.946471	8000.150532	12.178599	-0.078622	4.818321
397.340708	8000.106481	12.183603	-0.078696	4.818307
397.320780	8000.135636	12.188608	-0.078692	4.818315
397.429221	8000.076145	12.193613	-0.078712	4.818297
397.696657	8000.099741	12.198618	-0.078762	4.818303
397.189695	8000.168531	12.203623	-0.078668	4.818326
397.258081	8000.183119	12.208627	-0.078680	4.818330
397.149764	8000.256269	12.213632	-0.078660	4.818352
397.224176	8000.165836	12.218637	-0.078674	4.818325
397.383919	8000.119653	12.223642	-0.078704	4.818310
397.340004	8000.048635	12.228647	-0.078695	4.818290
398.097385	8000.016870	12.233651	-0.078836	4.818277
397.943136	8000.069427	12.238656	-0.078807	4.818293
397.731939	8000.015056	12.243661	-0.078768	4.818278
397.947519	8000.026387	12.248666	-0.078808	4.818280
397.575377	8000.079140	12.253671	-0.078739	4.818298
397.696114	8000.054499	12.258675	-0.078761	4.818290
397.389031	8000.104982	12.263680	-0.078704	4.818306
397.852051	8000.012466	12.268685	-0.078790	4.818277
398.150672	8000.033332	12.273690	-0.078846	4.818282
397.721395	8000.032757	12.278695	-0.078766	4.818283
397.190056	8000.187402	12.283699	-0.078667	4.818331
397.382831	8000.157433	12.288704	-0.078703	4.818322
396.945690	8000.128374	12.293709	-0.078621	4.818315
396.903242	8000.251816	12.298714	-0.078613	4.818352
397.121834	8000.188565	12.303719	-0.078654	4.818332
397.156188	8000.173262	12.308723	-0.078660	4.818327
397.067366	8000.185717	12.313728	-0.078644	4.818331
397.094984	8000.178731	12.318733	-0.078649	4.818329
397.099821	8000.153569	12.323738	-0.078650	4.818322
397.055442	8000.147708	12.328743	-0.078641	4.818320
397.070283	8000.183641	12.333747	-0.078644	4.818331
397.329182	8000.138804	12.338752	-0.078692	4.818316
397.066592	8000.112115	12.343757	-0.078643	4.818310
397.359146	8000.122388	12.348762	-0.078698	4.818311
397.846531	8000.007079	12.353767	-0.078788	4.818275
397.710807	8000.066194	12.358771	-0.078763	4.818293
398.096256	8000.017820	12.363776	-0.078835	4.818277
397.841529	7999.997542	12.368781	-0.078787	4.818272
398.117572	8000.017051	12.373786	-0.078839	4.818277
397.974248	8000.017205	12.378791	-0.078812	4.818278
397.736990	8000.050767	12.383795	-0.078768	4.818289
397.821314	8000.107614	12.388800	-0.078783	4.818305
397.930229	8000.039720	12.393805	-0.078804	4.818285
398.130410	8000.071864	12.398810	-0.078841	4.818293
398.044155	8000.091710	12.403815	-0.078825	4.818300
397.606772	8000.086821	12.408819	-0.078743	4.818300
397.929826	8000.088050	12.413824	-0.078803	4.818299
397.445750	8000.220212	12.418829	-0.078713	4.818340
397.513311	8000.208514	12.423834	-0.078726	4.818336
397.525598	8000.098318	12.428839	-0.078728	4.818304
397.878362	8000.084185	12.433843	-0.078794	4.818298
397.858311	8000.096522	12.438848	-0.078790	4.818302
397.782469	8000.075519	12.443853	-0.078776	4.818296
397.899227	8000.042416	12.448858	-0.078797	4.818285
397.938030	8000.013511	12.453863	-0.078805	4.818277
398.196690	7999.984436	12.458867	-0.078853	4.818267
397.846602	8000.023824	12.463872	-0.078787	4.818280
397.798979	8000.031583	12.468877	-0.078779	4.818283
398.187351	8000.038954	12.473882	-0.078851	4.818283
398.052775	8000.024511	12.478887	-0.078826	4.818280
397.871549	8000.052528	12.483891	-0.078792	4.818289
397.587967	8000.207382	12.488896	-0.078739	4.818336
397.740972	8000.072821	12.493901	-0.078768	4.818295
398.301043	8000.014204	12.498906	-0.078872	4.818275
397.993400	8000.029995	12.503911	-0.078814	4.818281
397.455092	8000.109921	12.508915	-0.078714	4.818307
397.711132	8000.133363	12.513920	-0.078762	4.818313
397.484965	8000.074585	12.518925	-0.078720	4.818297
397.377741	8000.217118	12.523930	-0.078700	4.818339
397.736748	8000.073791	12.528935	-0.078766	4.818295
397.895512	8000.060177	12.533939	-0.078796	4.818291
398.025620	8000.097676	12.538944	-0.078820	4.818301
397.468076	8000.112176	12.543949	-0.078716	4.818308
397.878004	8000.060981	12.548954	-0.078793	4.818291
397.489910	8000.083037	12.553959	-0.078720	4.818299
398.051533	8000.067534	12.558963	-0.078825	4.818292
397.967513	8000.047472	12.563968	-0.078809	4.818287
397.497937	8000.086289	12.568973	-0.078722	4.818300
397.826846	8000.061321	12.573978	-0.078783	4.818291
397.602806	8000.136054	12.578983	-0.078741	4.818315
397.719784	8000.092444	12.583987	-0.078763	4.818301
398.184654	8000.025178	12.588992	-0.078849	4.818279
398.128963	7999.972917	12.593997	-0.078839	4.818264
398.074109	8000.025773	12.599002	-0.078829	4.818280
398.510637	7999.949714	12.604007	-0.078910	4.818256
397.949838	8000.040896	12.609011	-0.078805	4.818285
398.105194	8000.050359	12.614016	-0.078834	4.818287
397.757679	8000.065608	12.619021	-0.078769	4.818293
398.186420	8000.073527	12.624026	-0.078849	4.818294
398.122334	8000.009591	12.629031	-0.078837	4.818275
398.269045	8000.011579	12.634035	-0.078865	4.818275
398.143850	8000.026693	12.639040	-0.078841	4.818280
398.172319	8000.045995	12.644045	-0.078846	4.818285
398.159379	8000.069990	12.649050	-0.078844	4.818293
397.955635	8000.041996	12.654055	-0.078806	4.818285
398.538057	8000.012062	12.659059	-0.078914	4.818274
398.342376	8000.015708	12.664064	-0.078878	4.818276
398.283078	8000.028563	12.669069	-0.078867	4.818280
398.354764	8000.035839	12.674074	-0.078880	4.818282
398.363380	8000.001268	12.679079	-0.078882	4.818271
397.821607	8000.075892	12.684083	-0.078781	4.818296
398.410409	8000.087036	12.689088	-0.078890	4.818297
398.348936	8000.047309	12.694093	-0.078879	4.818285
397.793701	8000.187965	12.699098	-0.078776	4.818329
397.662450	8000.136781	12.704103	-0.078751	4.818315
398.189257	8000.060897	12.709107	-0.078849	4.818290
398.507967	8000.008464	12.714112	-0.078908	4.818273
398.133177	8000.017036	12.719117	-0.078838	4.818277
398.320556	8000.061618	12.724122	-0.078873	4.818290
397.990070	8000.031903	12.729127	-0.078812	4.818282
397.644869	8000.059797	12.734131	-0.078747	4.818292
397.687244	8000.118176	12.739136	-0.078755	4.818309
397.750746	8000.068584	12.744141	-0.078767	4.818294
397.909304	8000.106469	12.749146	-0.078797	4.818305
397.953460	8000.045053	12.754151	-0.078805	4.818286
398.212153	8000.051715	12.759155	-0.078853	4.818287
397.817097	8000.116769	12.764160	-0.078779	4.818308
398.284240	8000.006441	12.769165	-0.078866	4.818273
398.551124	8000.015316	12.774170	-0.078916	4.818275
398.338616	7999.991407	12.779175	-0.078876	4.818269
397.679960	8000.039219	12.784179	-0.078754	4.818285
398.025764	8000.030246	12.789184	-0.078818	4.818281
398.440913	7999.977020	12.794189	-0.078895	4.818264
398.293829	7999.996041	12.799194	-0.078868	4.818270
398.365411	7999.958121	12.804199	-0.078881	4.818259
398.167922	8000.006938	12.809203	-0.078844	4.818274
398.345916	8000.015657	12.814208	-0.078877	4.818276
397.936116	8000.034265	12.819213	-0.078801	4.818283
398.330164	8000.029100	12.824218	-0.078874	4.818280
398.466423	7999.978394	12.829223	-0.078899	4.818264
398.333503	7999.992352	12.834227	-0.078875	4.818269
398.487570	8000.033329	12.839232	-0.078903	4.818280
398.153847	8000.000417	12.844237	-0.078841	4.818272
397.979183	8000.062157	12.849242	-0.078809	4.818291
397.518008	8000.095833	12.854247	-0.078723	4.818303
397.863077	8000.117330	12.859251	-0.078787	4.818308
397.967352	8000.117691	12.864256	-0.078806	4.818308
397.792554	8000.068018	12.869261	-0.078774	4.818294
397.958317	8000.128073	12.874266	-0.078805	4.818311
398.175012	8000.067948	12.879271	-0.078845	4.818292
397.780437	8000.100426	12.884275	-0.078771	4.818303
398.122895	8000.089306	12.889280	-0.078835	4.818299
398.577108	7999.990365	12.894285	-0.078920	4.818267
398.314094	8000.062466	12.899290	-0.078871	4.818290
397.994783	8000.095966	12.904295	-0.078811	4.818301
398.256575	8000.062730	12.909299	-0.078860	4.818290
398.711337	7999.994276	12.914304	-0.078944	4.818268
398.330523	8000.024838	12.919309	-0.078873	4.818279
398.477908	8000.036295	12.924314	-0.078901	4.818281
398.974872	7999.961058	12.929319	-0.078993	4.818257
398.968868	8000.001964	12.934323	-0.078992	4.818269
398.718583	8000.030094	12.939328	-0.078945	4.818279
398.393778	8000.008864	12.944333	-0.078885	4.818274
398.159165	8000.140210	12.949338	-0.078841	4.818314
398.115756	8000.141719	12.954343	-0.078833	4.818314
397.987245	8000.153634	12.959347	-0.078809	4.818318
398.246417	8000.165559	12.964352	-0.078857	4.818321
397.718029	8000.105829	12.969357	-0.078759	4.818305
397.845489	8000.181129	12.974362	-0.078783	4.818327
397.975291	8000.111417	12.979367	-0.078807	4.818306
397.854021	8000.112921	12.984371	-0.078784	4.818307
398.055992	8000.097791	12.989376	-0.078822	4.818301
398.345557	8000.071239	12.994381	-0.078876	4.818292
398.743004	8000.075582	12.999386	-0.078950	4.818292
399.062385	7999.981116	13.004391	-0.079009	4.818263
399.249211	7999.988905	13.009395	-0.079044	4.818264
399.194332	8000.003922	13.014400	-0.079033	4.818269
398.922340	7999.953979	13.019405	-0.078983	4.818255
399.075838	8000.000204	13.024410	-0.079011	4.818268
398.995470	7999.947608	13.029415	-0.078996	4.818253
398.501461	8000.020777	13.034419	-0.078904	4.818277
398.693237	8000.013918	13.039424	-0.078940	4.818274
398.469945	8000.024547	13.044429	-0.078898	4.818278
399.142111	7999.990577	13.049434	-0.079023	4.818265
398.567315	8000.023760	13.054439	-0.078916	4.818277
398.394522	8000.134924	13.059443	-0.078884	4.818311
398.141602	8000.114670	13.064448	-0.078837	4.818306
398.206866	8000.055643	13.069453	-0.078849	4.818288
398.143971	8000.115747	13.074458	-0.078837	4.818306
399.027545	7999.995308	13.079463	-0.079002	4.818267
398.558538	8000.050948	13.084467	-0.078914	4.818285
398.594675	8000.117652	13.089472	-0.078921	4.818305
398.366269	8000.107190	13.094477	-0.078879	4.818303
398.034556	8000.143674	13.099482	-0.078817	4.818315
398.005777	8000.209496	13.104487	-0.078811	4.818335
398.296192	8000.127250	13.109491	-0.078865	4.818309
398.227886	8000.213557	13.114496	-0.078853	4.818335
398.114374	8000.094294	13.119501	-0.078831	4.818300
398.536037	8000.073740	13.124506	-0.078910	4.818292
398.430138	8000.159536	13.129511	-0.078890	4.818318
397.951996	8000.212950	13.134515	-0.078801	4.818336
398.073985	8000.227216	13.139520	-0.078824	4.818340
397.984972	8000.181860	13.144525	-0.078807	4.818327
397.965468	8000.224685	13.149530	-0.078803	4.818339
397.941728	8000.138173	13.154535	-0.078799	4.818314
398.090080	8000.105499	13.159539	-0.078827	4.818304
398.729431	8000.067931	13.164544	-0.078945	4.818290
398.266417	8000.073202	13.169549	-0.078859	4.818293
398.689795	8000.086305	13.174554	-0.078938	4.818295
398.729284	8000.071072	13.179559	-0.078945	4.818291
398.836300	8000.029429	13.184563	-0.078965	4.818278
398.679676	8000.109281	13.189568	-0.078936	4.818302
398.389841	8000.082219	13.194573	-0.078882	4.818295
398.400177	8000.072897	13.199578	-0.078884	4.818293
398.174797	8000.096110	13.204583	-0.078842	4.818300
398.565191	8000.012067	13.209587	-0.078914	4.818274
398.285114	8000.191145	13.214592	-0.078862	4.818328
398.151840	8000.171464	13.219597	-0.078838	4.818323
397.968200	8000.200498	13.224602	-0.078803	4.818332
398.193389	8000.131030	13.229607	-0.078845	4.818311
398.090870	8000.149605	13.234611	-0.078826	4.818317
398.056427	8000.268954	13.239616	-0.078820	4.818352
397.999280	8000.153610	13.244621	-0.078809	4.818318
398.315716	8000.182078	13.249626	-0.078868	4.818325
398.234639	8000.234577	13.254631	-0.078853	4.818341
398.188800	8000.159326	13.259635	-0.078844	4.818319
397.993987	8000.214486	13.264640	-0.078808	4.818336
398.216061	8000.121852	13.269645	-0.078849	4.818308
398.234241	8000.109483	13.274650	-0.078852	4.818304
397.996479	8000.167212	13.279655	-0.078808	4.818322
398.086136	8000.092751	13.284659	-0.078825	4.818300
398.105712	8000.100371	13.289664	-0.078828	4.818302
398.562853	8000.010928	13.294669	-0.078913	4.818274
398.389116	8000.107365	13.299674	-0.078881	4.818303
398.513874	8000.063861	13.304679	-0.078904	4.818290
398.467790	8000.073742	13.309683	-0.078895	4.818293
398.493175	8000.076186	13.314688	-0.078900	4.818293
398.773074	8000.004307	13.319693	-0.078952	4.818271
398.533831	8000.066220	13.324698	-0.078908	4.818290
398.587854	8000.082717	13.329703	-0.078918	4.818295
398.554053	8000.108531	13.334707	-0.078911	4.818303
398.852462	8000.017984	13.339712	-0.078967	4.818275
398.724754	8000.009941	13.344717	-0.078943	4.818273
398.760239	8000.120780	13.349722	-0.078950	4.818305
398.526329	8000.126009	13.354727	-0.078906	4.818308
398.187356	8000.103535	13.359731	-0.078843	4.818303
398.226036	8000.147150	13.364736	-0.078850	4.818315
398.317205	8000.082168	13.369741	-0.078867	4.818296
398.376906	8000.108201	13.374746	-0.078878	4.818303
398.514063	8000.062763	13.379751	-0.078903	4.818289
398.916847	8000.016727	13.384755	-0.078978	4.818274
398.933842	8000.028516	13.389760	-0.078982	4.818277
398.911167	7999.981958	13.394765	-0.078977	4.818264
399.170008	7999.976010	13.399770	-0.079025	4.818261
399.109927	7999.980446	13.404775	-0.079014	4.818262
398.723548	8000.014085	13.409779	-0.078942	4.818274
399.087668	8000.011669	13.414784	-0.079010	4.818272
398.763813	8000.033545	13.419789	-0.078950	4.818280
398.959559	8000.060374	13.424794	-0.078986	4.818287
398.774963	8000.130387	13.429799	-0.078952	4.818308
399.070778	8000.032448	13.434803	-0.079007	4.818278
398.713149	8000.070682	13.439808	-0.078940	4.818291
398.717813	8000.042363	13.444813	-0.078941	4.818282
399.040757	8000.007856	13.449818	-0.079001	4.818271
399.138752	7999.998673	13.454823	-0.079019	4.818268
399.313511	7999.973715	13.459827	-0.079052	4.818260
398.959555	8000.047735	13.464832	-0.078986	4.818283
399.155663	8000.000995	13.469837	-0.079022	4.818268
399.358846	7999.991138	13.474842	-0.079060	4.818265
399.239111	7999.995815	13.479847	-0.079038	4.818266
399.234172	7999.964213	13.484851	-0.079037	4.818257
399.631619	7999.975914	13.489856	-0.079110	4.818259
399.205469	8000.002706	13.494861	-0.079031	4.818269
399.499236	8000.010897	13.499866	-0.079086	4.818270
399.491896	8000.006590	13.504871	-0.079084	4.818269
399.384661	8000.025100	13.509875	-0.079064	4.818275
399.645387	7999.997106	13.514880	-0.079113	4.818265
399.620807	7999.941062	13.519885	-0.079108	4.818249
399.568671	8000.010772	13.524890	-0.079098	4.818270
399.370093	8000.003868	13.529895	-0.079061	4.818268
399.101465	8000.025441	13.534899	-0.079011	4.818276
399.081955	8000.025173	13.539904	-0.079008	4.818276
399.080964	8000.040922	13.544909	-0.079008	4.818280
399.129379	8000.027913	13.549914	-0.079016	4.818276
399.039359	8000.038249	13.554919	-0.079000	4.818280
399.097841	8000.030631	13.559923	-0.079011	4.818277
398.693077	8000.159667	13.564928	-0.078935	4.818317
399.044917	8000.013089	13.569933	-0.079001	4.818272
399.148025	8000.024996	13.574938	-0.079020	4.818275
398.998253	8000.040827	13.579943	-0.078992	4.818281
398.625659	8000.088317	13.584947	-0.078922	4.818296
399.286822	8000.061557	13.589952	-0.079045	4.818286
399.215534	8000.026951	13.594957	-0.079032	4.818276
399.131739	8000.017401	13.599962	-0.079016	4.818273
399.404172	7999.997975	13.604967	-0.079067	4.818266
399.531328	7999.980779	13.609971	-0.079091	4.818261
399.366148	7999.990094	13.614976	-0.079060	4.818264
399.395087	7999.979973	13.619981	-0.079065	4.818261
399.640786	7999.993818	13.624986	-0.079111	4.818264
399.739478	7999.935244	13.629991	-0.079129	4.818246
399.705009	7999.920057	13.634995	-0.079123	4.818242
399.933548	7999.986223	13.640000	-0.079165	4.818261
399.345965	8000.027639	13.645005	-0.079056	4.818275
398.970245	8000.077188	13.650010	-0.078986	4.818292
399.008680	8000.018847	13.655015	-0.078993	4.818274
399.060192	8000.048973	13.660019	-0.079003	4.818283
399.377311	8000.046971	13.665024	-0.079062	4.818281
399.538318	7999.983988	13.670029	-0.079091	4.818262
399.469209	8000.037701	13.675034	-0.079079	4.818278
398.926867	8000.117571	13.680039	-0.078978	4.818304
398.597881	8000.071057	13.685043	-0.078916	4.818291
398.798002	8000.097946	13.690048	-0.078954	4.818299
398.445957	8000.157276	13.695053	-0.078888	4.818318
398.338243	8000.163168	13.700058	-0.078868	4.818320
398.675011	8000.130951	13.705063	-0.078931	4.818309
398.431810	8000.096113	13.710067	-0.078885	4.818300
398.554211	8000.172397	13.715072	-0.078908	4.818322
398.216496	8000.224565	13.720077	-0.078845	4.818339
398.480042	8000.229192	13.725082	-0.078894	4.818339
398.720605	8000.108430	13.730087	-0.078939	4.818302
398.888667	8000.118066	13.735091	-0.078970	4.818304
398.603756	8000.188819	13.740096	-0.078917	4.818326
399.028323	8000.056893	13.745101	-0.078996	4.818285
398.802391	8000.103221	13.750106	-0.078954	4.818300
399.218722	8000.048961	13.755111	-0.079031	4.818282
399.421451	8000.011771	13.760115	-0.079069	4.818270
399.258226	8000.046338	13.765120	-0.079039	4.818281
399.091182	7999.982053	13.770125	-0.079007	4.818263
399.404287	8000.004170	13.775130	-0.079066	4.818268
399.687427	7999.934438	13.780135	-0.079118	4.818246
399.539591	7999.958703	13.785139	-0.079091	4.818254
399.626715	7999.971445	13.790144	-0.079107	4.818258
399.197934	8000.001354	13.795149	-0.079027	4.818268
399.190570	8000.026477	13.800154	-0.079026	4.818276
399.751627	7999.993103	13.805159	-0.079130	4.818264
399.790093	7999.970498	13.810163	-0.079137	4.818257
399.440655	8000.041426	13.815168	-0.079072	4.818279
399.278378	8000.029758	13.820173	-0.079042	4.818276
400.000008	8000.002770	13.825178	-0.079176	4.818265
399.354093	8000.018167	13.830183	-0.079056	4.818273
398.968098	8000.017126	13.835187	-0.078984	4.818274
399.327181	8000.024102	13.840192	-0.079051	4.818275
399.046947	8000.030803	13.845197	-0.078998	4.818278
398.819075	8000.055033	13.850202	-0.078956	4.818286
398.951444	8000.037908	13.855207	-0.078981	4.818280
399.237435	8000.007103	13.860211	-0.079034	4.818270
399.580174	7999.998091	13.865216	-0.079098	4.818266
399.267011	8000.019060	13.870221	-0.079039	4.818273
399.424652	8000.064292	13.875226	-0.079069	4.818286
399.490580	8000.017886	13.880231	-0.079081	4.818272
399.114613	7999.995959	13.885235	-0.079011	4.818267
399.589334	8000.010812	13.890240	-0.079099	4.818270
399.162820	8000.021833	13.895245	-0.079020	4.818275
399.295373	8000.019426	13.900250	-0.079044	4.818273
399.436922	8000.066541	13.905255	-0.079071	4.818287
399.434159	8000.057041	13.910259	-0.079070	4.818284
399.363809	8000.068695	13.915264	-0.079057	4.818288
399.193267	8000.030639	13.920269	-0.079025	4.818277
399.000114	8000.075310	13.925274	-0.078989	4.818291
398.899561	8000.123341	13.930279	-0.078970	4.818306
398.762312	8000.079431	13.935283	-0.078945	4.818293
398.797456	8000.190267	13.940288	-0.078951	4.818326
399.093051	8000.050282	13.945293	-0.079006	4.818283
399.292983	7999.988879	13.950298	-0.079043	4.818264
399.208292	8000.010849	13.955303	-0.079027	4.818271
399.308239	8000.027969	13.960307	-0.079046	4.818276
398.972632	8000.091727	13.965312	-0.078984	4.818296
399.091702	7999.996643	13.970317	-0.079006	4.818267
399.464576	7999.993295	13.975322	-0.079075	4.818265
399.020986	8000.092374	13.980327	-0.078992	4.818296
399.204929	8000.010784	13.985331	-0.079027	4.818271
398.963410	8000.064258	13.990336	-0.078982	4.818288
399.220927	8000.002586	13.995341	-0.079029	4.818269
399.401310	8000.032360	14.000346	-0.079063	4.818277
399.253405	8000.031399	14.005351	-0.079035	4.818277
399.240529	7999.999689	14.010355	-0.079033	4.818268
399.108735	8000.013662	14.015360	-0.079008	4.818272
399.371284	7999.981488	14.020365	-0.079057	4.818262
399.102652	8000.064024	14.025370	-0.079007	4.818287
399.344680	8000.078870	14.030375	-0.079052	4.818291
399.507962	8000.016969	14.035379	-0.079083	4.818272
399.057286	8000.074960	14.040384	-0.078999	4.818291
398.844713	8000.106754	14.045389	-0.078959	4.818301
398.969378	8000.052738	14.050394	-0.078982	4.818285
398.997668	8000.078344	14.055399	-0.078987	4.818292
399.033819	8000.066219	14.060403	-0.078994	4.818288
399.290817	8000.085473	14.065408	-0.079042	4.818293
398.854062	8000.080588	14.070413	-0.078961	4.818293
399.292249	8000.077077	14.075418	-0.079042	4.818290
399.539045	8000.039434	14.080423	-0.079088	4.818278
399.653652	7999.969514	14.085427	-0.079109	4.818257
399.822603	8000.009645	14.090432	-0.079141	4.818268
399.821257	7999.969682	14.095437	-0.079140	4.818256
399.336992	8000.020910	14.100442	-0.079050	4.818274
399.465168	7999.989013	14.105447	-0.079074	4.818264
399.588158	7999.971761	14.110451	-0.079097	4.818258
399.680213	8000.012949	14.115456	-0.079114	4.818270
399.029079	8000.045094	14.120461	-0.078993	4.818282
399.253147	8000.063900	14.125466	-0.079034	4.818287
399.253903	8000.141686	14.130471	-0.079034	4.818310
399.462035	8000.027841	14.135475	-0.079073	4.818275
399.630882	8000.022774	14.140480	-0.079105	4.818273
399.383257	8000.046735	14.145485	-0.079058	4.818281
399.415928	8000.033511	14.150490	-0.079064	4.818277
399.400542	8000.030146	14.155495	-0.079061	4.818276
399.572848	7999.987287	14.160499	-0.079093	4.818263
399.587176	8000.027419	14.165504	-0.079096	4.818275
399.192860	8000.008396	14.170509	-0.079023	4.818270
399.408455	8000.022882	14.175514	-0.079063	4.818274
399.758083	8000.006607	14.180519	-0.079128	4.818268
399.317638	7999.985906	14.185523	-0.079046	4.818263
399.547732	8000.012151	14.190528	-0.079089	4.818270
399.881658	7999.953620	14.195533	-0.079151	4.818251
399.816058	7999.977951	14.200538	-0.079138	4.818259
399.102427	8000.036574	14.205543	-0.079006	4.818279
399.531924	7999.985647	14.210547	-0.079085	4.818262
399.744101	8000.033722	14.215552	-0.079125	4.818276
399.607631	8000.013996	14.220557	-0.079099	4.818270
399.892307	8000.014707	14.225562	-0.079152	4.818270
399.818433	8000.000036	14.230567	-0.079139	4.818265
399.696482	8000.008887	14.235571	-0.079116	4.818269
400.083811	7999.977358	14.240576	-0.079188	4.818258
399.768131	7999.954147	14.245581	-0.079129	4.818252
399.728114	7999.981979	14.250586	-0.079122	4.818261
399.489308	8000.023928	14.255591	-0.079077	4.818274
399.635397	8000.016449	14.260595	-0.079104	4.818271
399.384875	8000.097129	14.265600	-0.079058	4.818296
399.473377	8000.000578	14.270605	-0.079074	4.818267
399.226930	8000.055036	14.275610	-0.079028	4.818284
400.012865	8000.008951	14.280615	-0.079174	4.818267
400.092881	7999.949072	14.285619	-0.079189	4.818249
399.608939	8000.020274	14.290624	-0.079099	4.818272
399.206044	8000.034769	14.295629	-0.079024	4.818278
399.738223	7999.988390	14.300634	-0.079123	4.818262
400.027301	8000.003875	14.305639	-0.079177	4.818266
399.791328	7999.999615	14.310643	-0.079133	4.818265
400.181326	7999.976531	14.315648	-0.079205	4.818257
399.651347	8000.027137	14.320653	-0.079107	4.818274
399.784819	8000.008977	14.325658	-0.079131	4.818268
399.552861	8000.040508	14.330663	-0.079088	4.818279
399.577196	8000.020865	14.335667	-0.079093	4.818273
399.381294	8000.072856	14.340672	-0.079056	4.818289
399.278166	8000.055686	14.345677	-0.079037	4.818284
399.496241	8000.064951	14.350682	-0.079078	4.818286
399.858342	8000.025722	14.355687	-0.079145	4.818273
399.557565	8000.018479	14.360691	-0.079089	4.818272
399.608899	8000.062268	14.365696	-0.079098	4.818285
399.125070	8000.146084	14.370701	-0.079008	4.818312
399.354884	8000.072474	14.375706	-0.079051	4.818289
399.608677	8000.071714	14.380711	-0.079098	4.818288
399.407676	8000.038499	14.385715	-0.079061	4.818279
399.257551	8000.102675	14.390720	-0.079033	4.818298
399.348403	8000.053454	14.395725	-0.079050	4.818283
399.771052	8000.005587	14.400730	-0.079128	4.818267
399.546942	8000.047735	14.405735	-0.079086	4.818281
399.088453	8000.062526	14.410739	-0.079001	4.818287
399.487862	8000.082663	14.415744	-0.079075	4.818291
399.243486	7999.200667	14.420749	-0.079029	4.818030

399.432680	7996.069390	14.425754	-0.079062	4.817099
399.585273	7990.580789	14.430759	-0.079087	4.815468
399.390424	7984.006799	14.435763	-0.079047	4.813514
399.606329	7976.769164	14.440768	-0.079082	4.811361
399.612374	7969.160630	14.445773	-0.079078	4.809097
399.787299	7961.385856	14.450778	-0.079106	4.806782
399.255977	7953.511646	14.455783	-0.079002	4.804439
398.968410	7945.605718	14.460787	-0.078943	4.802085
399.375629	7937.570825	14.465792	-0.079013	4.799688
399.473461	7929.591590	14.470797	-0.079026	4.797308
399.343341	7921.582243	14.475802	-0.078997	4.794918
399.594649	7913.601193	14.480807	-0.079038	4.792535
399.646322	7905.508921	14.485811	-0.079043	4.790117
399.847748	7897.572778	14.490816	-0.079075	4.787745
399.436320	7889.553436	14.495821	-0.078993	4.785348
398.969149	7881.606542	14.500826	-0.078901	4.782973
398.661059	7873.681098	14.505831	-0.078838	4.780601
398.803979	7865.544447	14.510835	-0.078860	4.778164
398.910159	7857.567792	14.515840	-0.078874	4.775774
399.079933	7849.528050	14.520845	-0.078900	4.773364
398.924617	7841.531815	14.525850	-0.078866	4.770966
399.146926	7833.490224	14.530855	-0.078902	4.768552
399.055048	7825.557814	14.535859	-0.078880	4.766171
399.059690	7817.511834	14.540864	-0.078876	4.763754
399.311760	7809.537596	14.545869	-0.078917	4.761357
399.319184	7801.497663	14.550874	-0.078913	4.758940
399.142202	7793.613799	14.555879	-0.078875	4.756569
398.790523	7785.514698	14.560883	-0.078804	4.754132
398.779584	7777.623766	14.565888	-0.078797	4.751756
398.497529	7769.542970	14.570893	-0.078739	4.749322
398.530666	7761.521701	14.575898	-0.078740	4.746904
398.438118	7753.459057	14.580903	-0.078718	4.744473
398.699897	7745.525274	14.585907	-0.078761	4.742078
398.004677	7737.561617	14.590912	-0.078627	4.739675
397.829230	7729.545994	14.595917	-0.078589	4.737255
398.113668	7721.463323	14.600922	-0.078636	4.734811
398.052074	7713.523848	14.605927	-0.078620	4.732411
397.774012	7705.432279	14.610931	-0.078563	4.729963
397.640710	7697.508847	14.615936	-0.078532	4.727565
397.947160	7689.439618	14.620941	-0.078584	4.725121
397.728113	7681.545468	14.625946	-0.078538	4.722730
397.954989	7673.538502	14.630951	-0.078575	4.720302
397.830585	7665.483229	14.635955	-0.078547	4.717859
397.951912	7657.512680	14.640960	-0.078564	4.715440
397.725509	7649.549554	14.645965	-0.078517	4.713023
397.321950	7641.572277	14.650970	-0.078436	4.710600
397.417379	7633.553344	14.655975	-0.078449	4.708163
397.161138	7625.477422	14.660979	-0.078396	4.705707
397.390044	7617.474593	14.665984	-0.078433	4.703272
397.246211	7609.506081	14.670989	-0.078401	4.700847
397.416772	7601.518383	14.675994	-0.078428	4.698414
397.413608	7593.487002	14.680999	-0.078422	4.695966
397.470794	7585.436485	14.686003	-0.078427	4.693512
397.136254	7577.545408	14.691008	-0.078360	4.691105
396.930697	7569.532112	14.696013	-0.078316	4.688660
397.051591	7561.483163	14.701018	-0.078333	4.686202
397.211299	7553.475283	14.706023	-0.078358	4.683755
397.020367	7545.512499	14.711027	-0.078317	4.681321
396.897939	7537.528588	14.716032	-0.078289	4.678879
396.922198	7529.521680	14.721037	-0.078288	4.676429
396.705672	7521.506257	14.726042	-0.078243	4.673975
396.571342	7513.487132	14.731047	-0.078212	4.671519
396.230671	7505.446498	14.736051	-0.078144	4.669055
396.427254	7497.449677	14.741056	-0.078175	4.666602
396.525829	7489.355145	14.746061	-0.078188	4.664119
396.717705	7481.475456	14.751066	-0.078219	4.661700
396.887704	7473.423967	14.756071	-0.078245	4.659227
396.868838	7465.447677	14.761075	-0.078236	4.656776
396.616951	7457.445047	14.766080	-0.078184	4.654315
396.756413	7449.458008	14.771085	-0.078205	4.651858
396.602488	7441.401104	14.776090	-0.078171	4.649379
396.658420	7433.469144	14.781095	-0.078176	4.646936
396.146510	7425.460501	14.786099	-0.078075	4.644468
396.465565	7417.524716	14.791104	-0.078130	4.642022
396.121493	7409.430570	14.796109	-0.078060	4.639525
396.170619	7401.504399	14.801114	-0.078064	4.637079
396.211350	7393.462120	14.806119	-0.078066	4.634596
395.606836	7385.488643	14.811123	-0.077949	4.632132
395.987936	7377.378816	14.816128	-0.078014	4.629626
396.227383	7369.395595	14.821133	-0.078054	4.627157
396.238129	7361.327216	14.826138	-0.078050	4.624660
396.446199	7353.424083	14.831143	-0.078084	4.622213
395.750870	7345.431409	14.836147	-0.077949	4.619737
396.008027	7337.456041	14.841152	-0.077992	4.617265
395.898916	7329.349957	14.846157	-0.077966	4.614751
395.443691	7321.448510	14.851162	-0.077876	4.612299
395.853096	7313.357774	14.856167	-0.077947	4.609788
395.804803	7305.368249	14.861171	-0.077933	4.607306
396.344514	7297.338844	14.866176	-0.078028	4.604812
396.229287	7289.468551	14.871181	-0.078001	4.602364
395.858857	7281.389788	14.876186	-0.077927	4.599850
395.841740	7273.467579	14.881191	-0.077919	4.597384
395.928889	7265.366807	14.886195	-0.077930	4.594862
396.125808	7257.386157	14.891200	-0.077961	4.592375
396.113077	7249.318633	14.896205	-0.077953	4.589859
395.650778	7241.364760	14.901210	-0.077862	4.587377
395.616552	7233.353241	14.906215	-0.077850	4.584877
395.300867	7225.419535	14.911219	-0.077786	4.582398
395.399637	7217.329201	14.916224	-0.077800	4.579871
395.214795	7209.400622	14.921229	-0.077760	4.577391
395.149710	7201.321076	14.926234	-0.077742	4.574864
395.632775	7193.330506	14.931239	-0.077827	4.572364
395.712703	7185.241965	14.936243	-0.077837	4.569831
395.667055	7177.349937	14.941248	-0.077823	4.567358
395.612735	7169.300984	14.946253	-0.077808	4.564834
395.566496	7161.360934	14.951258	-0.077794	4.562344
395.760759	7153.367886	14.956263	-0.077825	4.559835
395.555373	7145.373075	14.961267	-0.077781	4.557324
395.685211	7137.283947	14.966272	-0.077800	4.554783
395.569352	7129.347082	14.971277	-0.077773	4.552288
394.696132	7121.400623	14.976282	-0.077606	4.549786
395.116352	7113.356421	14.981287	-0.077678	4.547255
394.605662	7105.335984	14.986291	-0.077578	4.544728
394.585662	7097.414209	14.991296	-0.077569	4.542232
393.931304	7089.362602	14.996301	-0.077442	4.539692
394.164638	7081.344660	15.001306	-0.077480	4.537164
394.323209	7073.302101	15.006311	-0.077504	4.534626
394.382779	7065.296518	15.011315	-0.077510	4.532098
394.719294	7057.222683	15.016320	-0.077568	4.529548
394.696824	7049.287976	15.021325	-0.077558	4.527039
394.781596	7041.245149	15.026330	-0.077569	4.524496
394.517039	7033.381855	15.031335	-0.077514	4.522006
394.299870	7025.287952	15.036339	-0.077469	4.519442
394.361509	7017.334770	15.041344	-0.077475	4.516923
394.224739	7009.294555	15.046349	-0.077444	4.514373
393.838879	7001.335388	15.051354	-0.077367	4.511847
393.827034	6993.299102	15.056359	-0.077359	4.509296
394.209487	6985.221752	15.061363	-0.077425	4.506733
394.520589	6977.178141	15.066368	-0.077478	4.504178
393.778139	6969.310037	15.071373	-0.077335	4.501674
393.950224	6961.224070	15.076378	-0.077361	4.499102
393.502707	6953.343153	15.081383	-0.077273	4.496592
392.962538	6945.294467	15.086387	-0.077167	4.494027
393.328628	6937.273834	15.091392	-0.077230	4.491472
393.660903	6929.191481	15.096397	-0.077286	4.488897
393.135172	6921.269229	15.101402	-0.077183	4.486367
393.891531	6913.153420	15.106407	-0.077319	4.483780
393.743418	6905.255040	15.111411	-0.077286	4.481257
393.544421	6897.216318	15.116416	-0.077244	4.478687
393.930259	6889.204750	15.121421	-0.077310	4.476127
393.713396	6881.210661	15.126426	-0.077265	4.473568
394.037686	6873.253782	15.131431	-0.077320	4.471023
393.828885	6865.209346	15.136435	-0.077276	4.468445
393.438540	6857.236483	15.141440	-0.077198	4.465888
393.241648	6849.240273	15.146445	-0.077156	4.463323
393.274088	6841.216235	15.151450	-0.077157	4.460749
392.874593	6833.282896	15.156455	-0.077077	4.458200
392.839556	6825.196286	15.161459	-0.077065	4.455602
393.281510	6817.162562	15.166464	-0.077142	4.453022
393.077722	6809.175228	15.171469	-0.077099	4.450452
393.152457	6801.132997	15.176474	-0.077108	4.447865
393.161634	6793.183696	15.181479	-0.077104	4.445305
392.989501	6785.164350	15.186483	-0.077067	4.442721
393.267061	6777.205459	15.191488	-0.077113	4.440157
393.192393	6769.236468	15.196493	-0.077094	4.437586
392.973522	6761.179729	15.201498	-0.077048	4.434985
393.066662	6753.200907	15.206503	-0.077060	4.432409
393.116391	6745.154978	15.211507	-0.077064	4.429810
392.646430	6737.264528	15.216512	-0.076971	4.427256
392.747480	6729.144178	15.221517	-0.076985	4.424630
392.655316	6721.181446	15.226522	-0.076962	4.422052
392.699847	6713.183408	15.231527	-0.076965	4.419462
392.035603	6705.217121	15.236531	-0.076837	4.416877
392.264032	6697.148254	15.241536	-0.076874	4.414262
392.402415	6689.192506	15.246541	-0.076894	4.411681
392.715517	6681.056442	15.251546	-0.076947	4.409042
392.875299	6673.109585	15.256551	-0.076972	4.406462
392.833963	6665.101002	15.261555	-0.076959	4.403859
392.999781	6657.173866	15.266560	-0.076984	4.401282
393.029443	6649.134988	15.271565	-0.076985	4.398666
392.782427	6641.170469	15.276570	-0.076933	4.396071
392.747461	6633.213320	15.281575	-0.076922	4.393479
392.936250	6625.130086	15.286579	-0.076952	4.390845
392.784119	6617.189526	15.291584	-0.076918	4.388254
392.635703	6609.182882	15.296589	-0.076885	4.385640
392.421252	6601.195803	15.301594	-0.076840	4.383031
392.387301	6593.240435	15.306599	-0.076828	4.380431
392.556837	6585.193954	15.311603	-0.076855	4.377801
392.153444	6577.236734	15.316608	-0.076774	4.375195
392.101919	6569.272231	15.321613	-0.076760	4.372588
392.289554	6561.159719	15.326618	-0.076789	4.369932
392.547158	6553.213411	15.331623	-0.076832	4.367329
392.377187	6545.175373	15.336627	-0.076795	4.364692
392.454296	6537.263368	15.341632	-0.076804	4.362097
392.359984	6529.218196	15.346637	-0.076781	4.359454
392.709733	6521.203210	15.351642	-0.076841	4.356824
392.356364	6513.220116	15.356647	-0.076770	4.354197
392.106858	6505.188399	15.361651	-0.076718	4.351553
391.782681	6497.218379	15.366656	-0.076653	4.348928
391.548132	6489.247453	15.371661	-0.076604	4.346301
391.758083	6481.165989	15.376666	-0.076638	4.343639
392.569446	6473.248531	15.381671	-0.076783	4.341035
392.049693	6465.190051	15.386675	-0.076681	4.338372
391.745601	6457.245047	15.391680	-0.076620	4.335747
391.845277	6449.210258	15.396685	-0.076633	4.333093
391.798760	6441.192394	15.401690	-0.076619	4.330443
391.762610	6433.236777	15.406695	-0.076607	4.327811
391.724378	6425.171960	15.411699	-0.076594	4.325142
391.911359	6417.253592	15.416704	-0.076624	4.322521
391.707610	6409.225385	15.421709	-0.076581	4.319860
391.653576	6401.229512	15.426714	-0.076566	4.317208
391.851611	6393.206786	15.431719	-0.076597	4.314548
391.615954	6385.267714	15.436723	-0.076548	4.311911
391.405913	6377.180729	15.441728	-0.076504	4.309223
391.635589	6369.197335	15.446733	-0.076541	4.306571
391.582374	6361.094790	15.451738	-0.076526	4.303876
391.365826	6353.242677	15.456743	-0.076480	4.301261
391.505088	6345.125433	15.461747	-0.076501	4.298559
391.729037	6337.176773	15.466752	-0.076538	4.295913
391.196089	6329.220540	15.471757	-0.076433	4.293255
391.036672	6321.146132	15.476762	-0.076398	4.290560
390.971373	6313.209863	15.481767	-0.076381	4.287910
390.852983	6305.180021	15.486771	-0.076353	4.285227
390.559928	6297.262814	15.491776	-0.076294	4.282578
390.591362	6289.211872	15.496781	-0.076294	4.279885
390.296172	6281.231120	15.501786	-0.076234	4.277211
390.288351	6273.205419	15.506791	-0.076227	4.274524
390.611921	6265.139948	15.511795	-0.076282	4.271824
390.863291	6257.126201	15.516800	-0.076324	4.269140
390.697446	6249.181534	15.521805	-0.076288	4.266472
390.400105	6241.171360	15.526810	-0.076227	4.263780
390.618560	6233.175442	15.531815	-0.076262	4.261096
390.809144	6225.140736	15.536819	-0.076293	4.258397
390.882419	6217.104324	15.541824	-0.076301	4.255695
390.494313	6209.165577	15.546829	-0.076223	4.253019
390.225500	6201.178368	15.551834	-0.076168	4.250326
390.624888	6193.135398	15.556839	-0.076237	4.247620
390.933009	6185.075187	15.561843	-0.076289	4.244905
390.646857	6177.184340	15.566848	-0.076231	4.242239
390.270074	6169.176582	15.571853	-0.076155	4.239532
390.303801	6161.174310	15.576858	-0.076156	4.236828
390.251618	6153.180743	15.581863	-0.076141	4.234125
390.429885	6145.147253	15.586867	-0.076169	4.231410
390.093643	6137.188574	15.591872	-0.076102	4.228712
389.919555	6129.211540	15.596877	-0.076064	4.226008
390.024543	6121.096338	15.601882	-0.076078	4.223258
389.906092	6113.181286	15.606887	-0.076051	4.220572
389.741804	6105.166139	15.611891	-0.076015	4.217850
390.017757	6097.127210	15.616896	-0.076061	4.215123
389.562904	6089.164142	15.621901	-0.075971	4.212412
389.787044	6081.078486	15.626906	-0.076008	4.209665
389.643554	6073.206484	15.631911	-0.075976	4.206985
389.342917	6065.120231	15.636915	-0.075914	4.204228
389.636191	6057.155077	15.641920	-0.075964	4.201518
389.810877	6049.119307	15.646925	-0.075991	4.198780
390.024394	6041.126735	15.651930	-0.076026	4.196056
390.115177	6033.073063	15.656935	-0.076037	4.193307
389.535550	6025.077778	15.661939	-0.075924	4.190569
389.354488	6017.124438	15.666944	-0.075885	4.187849
389.249317	6009.097985	15.671949	-0.075860	4.185102
389.257210	6001.111206	15.676954	-0.075856	4.182368
389.686048	5993.082088	15.681959	-0.075931	4.179623
389.117234	5985.186137	15.686963	-0.075820	4.176910
388.881970	5977.157237	15.691968	-0.075771	4.174154
389.514872	5969.111892	15.696973	-0.075883	4.171401
389.545965	5961.068637	15.701978	-0.075884	4.168639
389.134734	5953.157450	15.706983	-0.075802	4.165915
389.077752	5945.128048	15.711987	-0.075786	4.163153
389.318354	5937.136704	15.716992	-0.075826	4.160407
389.277470	5929.156321	15.721997	-0.075813	4.157658
388.810735	5921.152529	15.727002	-0.075721	4.154895
389.040989	5913.183689	15.732007	-0.075758	4.152150
389.036804	5905.092156	15.737011	-0.075752	4.149359
388.983944	5897.142593	15.742016	-0.075737	4.146613
389.274568	5889.066166	15.747021	-0.075786	4.143827
388.735198	5881.216001	15.752026	-0.075680	4.141106
388.848655	5873.165996	15.757031	-0.075696	4.138323
388.595540	5865.155193	15.762035	-0.075644	4.135547
388.425245	5857.194457	15.767040	-0.075607	4.132787
388.455180	5849.212488	15.772045	-0.075607	4.130020
388.636707	5841.138214	15.777050	-0.075636	4.127222
388.343892	5833.130080	15.782055	-0.075576	4.124438
388.511259	5825.186746	15.787059	-0.075602	4.121682
388.627113	5817.148325	15.792064	-0.075618	4.118889
388.648384	5809.201608	15.797069	-0.075617	4.116126
388.210250	5801.192385	15.802074	-0.075530	4.113332
388.108822	5793.196863	15.807079	-0.075506	4.110546
387.707049	5785.188409	15.812083	-0.075426	4.107749
387.074099	5777.218168	15.817088	-0.075303	4.104961
387.094889	5769.244131	15.822093	-0.075301	4.102178
386.732029	5761.188345	15.827098	-0.075228	4.099360
386.937833	5753.221278	15.832103	-0.075262	4.096578
387.315733	5745.090054	15.837107	-0.075327	4.093740
387.218737	5737.100746	15.842112	-0.075303	4.090943
387.258286	5729.148718	15.847117	-0.075305	4.088159
387.075572	5721.128533	15.852122	-0.075266	4.085345
387.290425	5713.173854	15.857127	-0.075301	4.082559
387.346002	5705.111157	15.862131	-0.075306	4.079730
387.716745	5697.123377	15.867136	-0.075370	4.076931
387.457055	5689.134827	15.872141	-0.075316	4.074120
387.521105	5681.151419	15.877146	-0.075323	4.071314
387.266266	5673.176508	15.882151	-0.075270	4.068503
387.227240	5665.121716	15.887155	-0.075258	4.065666
387.049918	5657.147629	15.892160	-0.075219	4.062854
387.521676	5649.109375	15.897165	-0.075302	4.060027
387.214160	5641.191873	15.902170	-0.075239	4.057228
386.991748	5633.188743	15.907175	-0.075193	4.054398
387.086105	5625.169419	15.912179	-0.075205	4.051566
387.044598	5617.127253	15.917184	-0.075192	4.048722
386.898405	5609.151853	15.922189	-0.075159	4.045897
386.800730	5601.154370	15.927194	-0.075136	4.043064
386.477301	5593.262480	15.932199	-0.075071	4.040262
387.146610	5585.167001	15.937203	-0.075190	4.037402
386.925899	5577.164657	15.942208	-0.075144	4.034559
386.732618	5569.169447	15.947213	-0.075102	4.031717
387.032378	5561.050369	15.952218	-0.075153	4.028836
387.139917	5553.104617	15.957223	-0.075168	4.026012
387.114687	5545.112616	15.962227	-0.075158	4.023168
386.945399	5537.133804	15.967232	-0.075121	4.020324
387.149722	5529.178446	15.972237	-0.075154	4.017492
387.054550	5521.124402	15.977242	-0.075131	4.014618
386.510696	5513.252785	15.982247	-0.075024	4.011800
386.417299	5505.215506	15.987251	-0.075002	4.008928
386.282777	5497.213913	15.992256	-0.074971	4.006066
386.942084	5489.139559	15.997261	-0.075089	4.003190
386.269899	5481.226376	16.002266	-0.074958	4.000346
386.675346	5473.211107	16.007271	-0.075029	3.997482
386.360646	5465.228044	16.012275	-0.074965	3.994616
386.419179	5457.204205	16.017280	-0.074970	3.991739
386.327955	5449.212486	16.022285	-0.074948	3.988869
386.235417	5441.191874	16.027290	-0.074926	3.985986
386.315149	5433.181755	16.032295	-0.074935	3.983108
385.999588	5425.234875	16.037299	-0.074871	3.980244
386.292476	5417.215478	16.042304	-0.074920	3.977362
385.582294	5409.282329	16.047309	-0.074783	3.974492
385.293570	5401.258214	16.052314	-0.074724	3.971594
385.576148	5393.190119	16.057319	-0.074771	3.968689
385.673569	5385.178534	16.062323	-0.074784	3.965798
385.367998	5377.259415	16.067328	-0.074722	3.962931
385.594367	5369.202938	16.072333	-0.074759	3.960023
385.825538	5361.189139	16.077338	-0.074797	3.957127
385.631441	5353.202621	16.082343	-0.074755	3.954232
385.773617	5345.211000	16.087347	-0.074777	3.951339
385.424178	5337.250230	16.092352	-0.074706	3.948446
385.496004	5329.186181	16.097357	-0.074714	3.945521
385.278800	5321.244336	16.102362	-0.074669	3.942632
385.219878	5313.222964	16.107367	-0.074652	3.939716
385.541590	5305.209325	16.112371	-0.074707	3.936808
385.378648	5297.183771	16.117376	-0.074671	3.933884
384.975597	5289.241038	16.122381	-0.074591	3.930983
384.976441	5281.209584	16.127386	-0.074586	3.928055
384.423953	5273.342368	16.132391	-0.074478	3.925175
384.591939	5265.237162	16.137395	-0.074504	3.922219
384.637193	5257.227357	16.142400	-0.074507	3.919294
384.966271	5249.234913	16.147405	-0.074563	3.916378
384.847603	5241.164669	16.152410	-0.074536	3.913424
385.239167	5233.178983	16.157415	-0.074603	3.910507
385.338096	5225.170511	16.162419	-0.074617	3.907575
385.352109	5217.134291	16.167424	-0.074614	3.904628
385.385583	5209.279127	16.172429	-0.074615	3.901746
384.831879	5201.295051	16.177434	-0.074507	3.898803
385.108054	5193.289898	16.182439	-0.074553	3.895867
384.523943	5185.325795	16.187443	-0.074439	3.892926
384.408149	5177.280395	16.192448	-0.074412	3.889962
384.334817	5169.348984	16.197453	-0.074393	3.887039
384.065341	5161.274408	16.202458	-0.074338	3.884057
384.428429	5153.355512	16.207463	-0.074400	3.881143
384.224672	5145.329392	16.212467	-0.074357	3.878175
384.117829	5137.346334	16.217472	-0.074332	3.875223
383.618915	5129.277430	16.222477	-0.074233	3.872229
383.912158	5121.119032	16.227482	-0.074283	3.869216
383.571821	5113.274778	16.232487	-0.074214	3.866304
383.467108	5105.252322	16.237491	-0.074189	3.863328
383.345328	5097.322887	16.242496	-0.074161	3.860385
383.465184	5089.308447	16.247501	-0.074178	3.857412
383.591297	5081.205694	16.252506	-0.074197	3.854405
383.661164	5073.297116	16.257511	-0.074204	3.851466
383.407514	5065.296578	16.262515	-0.074152	3.848484
383.376137	5057.294552	16.267520	-0.074141	3.845504
383.199970	5049.349850	16.272525	-0.074103	3.842539
383.166748	5041.283385	16.277530	-0.074091	3.839530
383.329200	5033.337278	16.282535	-0.074116	3.836568
383.359874	5025.293831	16.287539	-0.074117	3.833565
383.337001	5017.242293	16.292544	-0.074107	3.830554
383.097105	5009.354203	16.297549	-0.074057	3.827598
382.977395	5001.245156	16.302554	-0.074030	3.824559
383.412252	4993.292965	16.307559	-0.074106	3.821589
382.795632	4985.387685	16.312563	-0.073986	3.818611
382.570055	4977.390665	16.317568	-0.073938	3.815605
382.748230	4969.360921	16.322573	-0.073966	3.812593
382.719122	4961.286802	16.327578	-0.073955	3.809558
382.642389	4953.324049	16.332583	-0.073936	3.806561
382.507015	4945.318929	16.337587	-0.073905	3.803544
382.101626	4937.392926	16.342592	-0.073825	3.800548
382.136242	4929.413478	16.347597	-0.073826	3.797540
381.921003	4921.389436	16.352602	-0.073781	3.794507
382.265583	4913.324410	16.357607	-0.073839	3.791469
382.227417	4905.323067	16.362611	-0.073827	3.788444
382.108495	4897.333115	16.367616	-0.073800	3.785419
381.921130	4889.399177	16.372621	-0.073760	3.782411
382.204613	4881.304890	16.377626	-0.073807	3.779351
381.898326	4873.440547	16.382631	-0.073745	3.776361
381.793862	4865.376728	16.387635	-0.073720	3.773299
381.689324	4857.363883	16.392640	-0.073695	3.770253
381.656494	4849.380156	16.397645	-0.073684	3.767217
381.084573	4841.421250	16.402650	-0.073572	3.764176
381.109214	4833.477248	16.407655	-0.073572	3.761152
381.200409	4825.433038	16.412659	-0.073583	3.758089
381.940309	4817.296838	16.417664	-0.073716	3.755004
381.859368	4809.398406	16.422669	-0.073695	3.751988
381.625794	4801.410733	16.427674	-0.073647	3.748931
381.383432	4793.456369	16.432679	-0.073596	3.745884
381.489480	4785.389928	16.437683	-0.073611	3.742800
381.629242	4777.362148	16.442688	-0.073632	3.739730
381.394692	4769.496238	16.447693	-0.073583	3.736710
381.570138	4761.392934	16.452698	-0.073610	3.733606
382.076486	4753.314589	16.457703	-0.073699	3.730518
382.001569	4745.357031	16.462707	-0.073680	3.727459
381.802832	4737.401168	16.467712	-0.073638	3.724395
382.030310	4729.469364	16.472717	-0.073675	3.721349
381.862891	4721.458152	16.477722	-0.073638	3.718259
382.067112	4713.472036	16.482727	-0.073671	3.715186
381.902798	4705.434349	16.487731	-0.073635	3.712081
381.504289	4697.421455	16.492736	-0.073556	3.708977
381.298456	4689.472064	16.497741	-0.073512	3.705900
381.364853	4681.416763	16.502746	-0.073519	3.702787
381.417324	4673.470736	16.507751	-0.073524	3.699712
381.366683	4665.478616	16.512755	-0.073509	3.696615
381.536668	4657.430858	16.517760	-0.073536	3.693499
381.167749	4649.497034	16.522765	-0.073462	3.690411
381.111931	4641.471648	16.527770	-0.073446	3.687293
381.018865	4633.474883	16.532775	-0.073423	3.684182
380.978576	4625.548704	16.537779	-0.073411	3.681097
380.871997	4617.490257	16.542784	-0.073385	3.677957
381.108643	4609.484074	16.547789	-0.073424	3.674843
381.016066	4601.489620	16.552794	-0.073402	3.671723
380.689608	4593.550120	16.557799	-0.073336	3.668615
380.396134	4585.595249	16.562803	-0.073276	3.665499
380.348822	4577.617433	16.567808	-0.073262	3.662379
380.132068	4569.584870	16.572813	-0.073216	3.659229
380.002611	4561.625737	16.577818	-0.073187	3.656108
380.261258	4553.576266	16.582823	-0.073230	3.652960
380.229270	4545.538900	16.587827	-0.073219	3.649805
380.331427	4537.514166	16.592832	-0.073232	3.646656
380.310228	4529.560600	16.597837	-0.073223	3.643530
380.116256	4521.568187	16.602842	-0.073182	3.640380
380.040314	4513.633857	16.607847	-0.073162	3.637254
379.975325	4505.586823	16.612851	-0.073145	3.634081
379.729940	4497.627760	16.617856	-0.073094	3.630935
379.782866	4489.581653	16.622861	-0.073099	3.627761
379.877018	4481.515922	16.627866	-0.073111	3.624576
380.344670	4473.550343	16.632871	-0.073193	3.621440
380.091982	4465.581881	16.637875	-0.073140	3.618279
380.045325	4457.574101	16.642880	-0.073126	3.615105
379.758639	4449.656101	16.647885	-0.073068	3.611958
380.060851	4441.562373	16.652890	-0.073119	3.608754
379.790731	4433.634463	16.657895	-0.073063	3.605598
379.241094	4425.730900	16.662899	-0.072956	3.602440
379.366225	4417.654124	16.667904	-0.072974	3.599230
379.369216	4409.705526	16.672909	-0.072969	3.596064
379.454924	4401.612221	16.677914	-0.072980	3.592841
379.275797	4393.682581	16.682919	-0.072941	3.589672
379.863414	4385.596214	16.687923	-0.073045	3.586461
379.415963	4377.659227	16.692928	-0.072957	3.583275
378.981581	4369.730874	16.697933	-0.072871	3.580091
379.211517	4361.680722	16.702938	-0.072908	3.576874
379.489884	4353.655895	16.707943	-0.072955	3.573667
379.320303	4345.685743	16.712947	-0.072918	3.570465
379.383083	4337.683592	16.717952	-0.072924	3.567254
379.323798	4329.690832	16.722957	-0.072908	3.564041
379.242178	4321.717087	16.727962	-0.072888	3.560831
379.481827	4313.728563	16.732967	-0.072927	3.557623
379.328542	4305.735935	16.737971	-0.072893	3.554398
378.879768	4297.720518	16.742976	-0.072804	3.551152
378.648420	4289.777991	16.747981	-0.072756	3.547938
379.110489	4281.625957	16.752986	-0.072837	3.544659
378.773126	4273.777957	16.757991	-0.072769	3.541475
378.562736	4265.783234	16.762995	-0.072724	3.538232
379.145364	4257.655455	16.768000	-0.072827	3.534958
379.112208	4249.727224	16.773005	-0.072816	3.531742
379.057811	4241.707930	16.778010	-0.072801	3.528485
378.999269	4233.712523	16.783015	-0.072785	3.525235
379.208862	4225.785754	16.788019	-0.072818	3.522019
379.022081	4217.759839	16.793024	-0.072778	3.518746
378.756173	4209.841127	16.798029	-0.072724	3.515512
378.588956	4201.839435	16.803034	-0.072687	3.512244
378.990853	4193.753103	16.808039	-0.072757	3.508956
378.945269	4185.798063	16.813043	-0.072743	3.505705
378.742073	4177.806413	16.818048	-0.072700	3.502431
379.045777	4169.773020	16.823053	-0.072751	3.499152
378.940388	4161.831313	16.828058	-0.072726	3.495896
379.003024	4153.832694	16.833063	-0.072733	3.492618
378.790029	4145.826306	16.838067	-0.072688	3.489325
378.636883	4137.891152	16.843072	-0.072654	3.486060
378.522334	4129.894392	16.848077	-0.072627	3.482768
378.689216	4121.850025	16.853082	-0.072653	3.479462
378.495146	4113.915790	16.858087	-0.072612	3.476187
378.140883	4105.971044	16.863091	-0.072541	3.472899
378.201061	4097.911224	16.868096	-0.072547	3.469574
378.161365	4089.920838	16.873101	-0.072534	3.466271
377.993913	4081.903970	16.878106	-0.072498	3.462950
377.914167	4073.926165	16.883111	-0.072477	3.459644
378.362759	4065.912079	16.888115	-0.072556	3.456339
378.409189	4057.865434	16.893120	-0.072559	3.453003
378.278867	4049.936525	16.898125	-0.072530	3.449707
378.018836	4041.962862	16.903130	-0.072476	3.446384
378.463491	4033.898348	16.908135	-0.072553	3.443045
377.996057	4026.012085	16.913139	-0.072461	3.439745
378.205046	4017.995915	16.918144	-0.072495	3.436412
378.261540	4010.008332	16.923149	-0.072500	3.433082
378.181095	4001.990565	16.928154	-0.072480	3.429731
377.616076	3994.103256	16.933159	-0.072369	3.426414
377.812109	3986.031134	16.938163	-0.072401	3.423044
377.831374	3978.013742	16.943168	-0.072399	3.419687
377.837196	3970.050010	16.948173	-0.072395	3.416348
377.871727	3961.982332	16.953178	-0.072396	3.412964
378.218174	3953.952759	16.958183	-0.072455	3.409603
377.835507	3946.046845	16.963187	-0.072379	3.406266
377.923906	3938.022890	16.968192	-0.072390	3.402892
377.848411	3930.088197	16.973197	-0.072371	3.399546
377.915733	3922.090725	16.978202	-0.072378	3.396176
377.743726	3914.072821	16.983207	-0.072341	3.392785
377.716758	3906.053555	16.988211	-0.072330	3.389396
377.951373	3898.013978	16.993216	-0.072369	3.386004
377.751126	3890.085346	16.998221	-0.072326	3.382639
377.435459	3882.123849	17.003226	-0.072262	3.379254
377.440674	3874.161149	17.008231	-0.072258	3.375876
377.279092	3866.173839	17.013235	-0.072223	3.372478
377.260336	3858.128681	17.018240	-0.072214	3.369057
377.478452	3850.154699	17.023245	-0.072249	3.365672
377.315677	3842.171298	17.028250	-0.072214	3.362265
377.171221	3834.201055	17.033255	-0.072182	3.358861
377.310144	3826.203187	17.038259	-0.072202	3.355452
377.115989	3818.225816	17.043264	-0.072161	3.352037
377.119909	3810.206422	17.048269	-0.072156	3.348607
376.792745	3802.244107	17.053274	-0.072090	3.345185
377.023376	3794.219713	17.058279	-0.072128	3.341755
377.289709	3786.197384	17.063283	-0.072172	3.338323
377.077302	3778.217661	17.068288	-0.072127	3.334888
377.291610	3770.238811	17.073293	-0.072162	3.331466
377.093861	3762.240246	17.078298	-0.072120	3.328016
376.923582	3754.282387	17.083303	-0.072083	3.324581
376.906733	3746.343709	17.088307	-0.072075	3.321157
376.688853	3738.348136	17.093312	-0.072029	3.317697
376.653509	3730.319335	17.098317	-0.072017	3.314226
376.659670	3722.318309	17.103322	-0.072013	3.310765
376.542782	3714.330994	17.108327	-0.071986	3.307301
376.188350	3706.344804	17.113331	-0.071914	3.303825
375.851168	3698.400143	17.118336	-0.071846	3.300364
375.914868	3690.419662	17.123341	-0.071853	3.296900
375.264591	3682.489585	17.128346	-0.071727	3.293425
375.206693	3674.422407	17.133351	-0.071711	3.289911
375.329213	3666.425425	17.138355	-0.071728	3.286430
375.615692	3658.358183	17.143360	-0.071776	3.282922
375.102475	3650.498598	17.148365	-0.071676	3.279469
375.717831	3642.383837	17.153370	-0.071785	3.275946
375.917140	3634.371478	17.158375	-0.071817	3.272447
375.688299	3626.423536	17.163379	-0.071769	3.268955
375.234638	3618.479406	17.168384	-0.071679	3.265452
375.178830	3610.541221	17.173389	-0.071664	3.261965
375.102053	3602.508446	17.178394	-0.071644	3.258430
375.155852	3594.504880	17.183399	-0.071649	3.254911
375.186652	3586.492972	17.188403	-0.071649	3.251383
375.519538	3578.452995	17.193408	-0.071706	3.247851
375.382399	3570.517973	17.198413	-0.071675	3.244342
375.425093	3562.535881	17.203418	-0.071678	3.240816
375.369228	3554.591483	17.208423	-0.071662	3.237299
375.379287	3546.584719	17.213427	-0.071659	3.233753
375.149293	3538.599575	17.218432	-0.071611	3.230202
375.250528	3530.583519	17.223437	-0.071624	3.226648
375.197770	3522.574714	17.228442	-0.071609	3.223087
374.986213	3514.599011	17.233447	-0.071565	3.219530
375.196800	3506.590600	17.238451	-0.071599	3.215972
374.929559	3498.626082	17.243456	-0.071544	3.212409
374.843126	3490.635058	17.248461	-0.071522	3.208839
374.972146	3482.592518	17.253466	-0.071541	3.205250
374.848114	3474.685066	17.258471	-0.071513	3.201707
374.963486	3466.672117	17.263475	-0.071529	3.198124
374.502554	3458.724381	17.268480	-0.071438	3.194540
374.889077	3450.689289	17.273485	-0.071504	3.190950
374.766119	3442.692255	17.278490	-0.071476	3.187351
374.252271	3434.750573	17.283495	-0.071375	3.183756
374.741248	3426.717842	17.288499	-0.071461	3.180159
374.823498	3418.721820	17.293504	-0.071471	3.176557
374.523474	3410.797030	17.298509	-0.071410	3.172967
373.887505	3402.836205	17.303514	-0.071287	3.169341
374.391980	3394.784075	17.308519	-0.071375	3.165720
374.080788	3386.846492	17.313523	-0.071312	3.162111
374.015584	3378.853334	17.318528	-0.071295	3.158483
373.681534	3370.941944	17.323533	-0.071227	3.154876
373.961715	3362.840434	17.328538	-0.071274	3.151206
373.753953	3354.880853	17.333543	-0.071230	3.147575
373.853825	3346.865130	17.338547	-0.071243	3.143927
373.874215	3338.848089	17.343552	-0.071242	3.140271
374.261236	3330.850341	17.348557	-0.071309	3.136637
373.581055	3322.931266	17.353562	-0.071177	3.132985
373.767825	3314.893544	17.358567	-0.071206	3.129315
373.382824	3306.995948	17.363571	-0.071130	3.125678
373.488109	3298.953140	17.368576	-0.071144	3.121993
373.347991	3291.008298	17.373581	-0.071113	3.118337
373.352420	3282.993154	17.378586	-0.071108	3.114651
373.262810	3275.026806	17.383591	-0.071086	3.110979
373.153094	3267.034039	17.388595	-0.071061	3.107289
372.624630	3259.121635	17.393600	-0.070957	3.103613
373.235969	3251.031625	17.398605	-0.071065	3.099903
372.912214	3243.075747	17.403610	-0.071000	3.096207
372.813315	3235.098544	17.408615	-0.070976	3.092508
372.617871	3227.130030	17.413619	-0.070935	3.088803
372.760659	3219.076108	17.418624	-0.070956	3.085071
372.829230	3211.133434	17.423629	-0.070963	3.081382
373.210267	3203.079004	17.428634	-0.071029	3.077651
373.289416	3195.108046	17.433639	-0.071039	3.073941
372.966238	3187.121919	17.438643	-0.070973	3.070199
373.141402	3179.084233	17.443648	-0.071001	3.066453
373.457014	3171.091792	17.448653	-0.071054	3.062730
373.317543	3163.142068	17.453658	-0.071023	3.059001
373.003867	3155.225520	17.458663	-0.070959	3.055275
373.009265	3147.233099	17.463667	-0.070955	3.051523
372.720962	3139.230653	17.468672	-0.070896	3.047748
372.877451	3131.244224	17.473677	-0.070920	3.043998
372.765183	3123.291691	17.478682	-0.070894	3.040245
372.688092	3115.341383	17.483687	-0.070874	3.036491
372.421723	3107.397034	17.488691	-0.070819	3.032726
372.160183	3099.367839	17.493696	-0.070765	3.028915
372.480135	3091.348243	17.498701	-0.070820	3.025134
372.263166	3083.391890	17.503706	-0.070774	3.021351
372.491600	3075.343966	17.508711	-0.070811	3.017542
372.748623	3067.347039	17.513715	-0.070854	3.013754
372.375940	3059.395392	17.518720	-0.070779	3.009951
372.544704	3051.404937	17.523725	-0.070805	3.006153
372.286057	3043.470020	17.528730	-0.070752	3.002354
372.366293	3035.443155	17.533735	-0.070762	2.998523
372.175189	3027.522047	17.538739	-0.070721	2.994725
372.318023	3019.499758	17.543744	-0.070742	2.990890
372.462477	3011.493366	17.548749	-0.070764	2.987058
372.292765	3003.515994	17.553754	-0.070727	2.983219
372.382064	2995.512009	17.558759	-0.070738	2.979376
372.098397	2987.622051	17.563763	-0.070680	2.975563
372.296985	2979.576325	17.568768	-0.070712	2.971695
372.287506	2971.589996	17.573773	-0.070705	2.967840
372.324383	2963.570934	17.578778	-0.070707	2.963966
372.149656	2955.663983	17.583783	-0.070669	2.960131
371.851448	2947.751835	17.588787	-0.070608	2.956281
371.530144	2939.754280	17.593792	-0.070543	2.952384
372.011008	2931.659297	17.598797	-0.070627	2.948477
371.401929	2923.762664	17.603802	-0.070509	2.944603
371.927167	2915.691574	17.608807	-0.070601	2.940700
371.747691	2907.779299	17.613811	-0.070563	2.936831
371.373635	2899.808236	17.618816	-0.070488	2.932918
371.723762	2891.767581	17.623821	-0.070548	2.929005
371.394469	2883.851978	17.628826	-0.070481	2.925110
371.436589	2875.884393	17.633831	-0.070484	2.921206
371.232360	2867.910883	17.638835	-0.070440	2.917280
371.400900	2859.871956	17.643840	-0.070467	2.913336
371.372637	2851.825777	17.648845	-0.070456	2.909373
371.278280	2843.875772	17.653850	-0.070433	2.905448
371.224621	2835.914957	17.658855	-0.070418	2.901515
371.049378	2827.968453	17.663859	-0.070380	2.897577
371.359529	2819.874532	17.668864	-0.070433	2.893588
371.232998	2811.955110	17.673869	-0.070404	2.889655
371.405463	2803.947593	17.678874	-0.070431	2.885690
371.069248	2796.063448	17.683879	-0.070363	2.881752
371.253038	2788.046418	17.688883	-0.070392	2.877771
370.880156	2780.076932	17.693888	-0.070317	2.873778
371.316900	2772.049676	17.698893	-0.070393	2.869796
370.754484	2764.152118	17.703898	-0.070283	2.865817
370.717950	2756.171261	17.708903	-0.070271	2.861820
370.842597	2748.165204	17.713907	-0.070289	2.857814
370.380617	2740.255117	17.718912	-0.070198	2.853817
370.306710	2732.255624	17.723917	-0.070179	2.849792
370.200962	2724.274210	17.728922	-0.070154	2.845768
370.016282	2716.306985	17.733927	-0.070114	2.841742
370.039797	2708.332851	17.738931	-0.070114	2.837718
369.761869	2700.367598	17.743936	-0.070057	2.833675
369.658833	2692.404841	17.748941	-0.070032	2.829638
369.069668	2684.447357	17.753946	-0.069917	2.825569
369.317342	2676.389111	17.758951	-0.069958	2.821493
369.461947	2668.392331	17.763955	-0.069980	2.817435
369.608664	2660.360792	17.768960	-0.070002	2.813355
369.481600	2652.391543	17.773965	-0.069973	2.809283
369.203948	2644.459964	17.778970	-0.069916	2.805217
369.357816	2636.481284	17.783975	-0.069939	2.801146
369.143499	2628.538149	17.788979	-0.069894	2.797065
368.919365	2620.540352	17.793984	-0.069847	2.792949
369.211320	2612.532985	17.798989	-0.069896	2.788854
369.014134	2604.553273	17.803994	-0.069854	2.784737
368.760065	2596.635140	17.808999	-0.069802	2.780643
368.944096	2588.624112	17.814003	-0.069831	2.776521
369.365712	2580.570342	17.819008	-0.069904	2.772385
368.965546	2572.663831	17.824013	-0.069824	2.768269
368.595209	2564.730864	17.829018	-0.069750	2.764136
368.677485	2556.764845	17.834023	-0.069760	2.760006
368.394361	2548.839591	17.839027	-0.069702	2.755869
368.278651	2540.777686	17.844032	-0.069675	2.751665
368.266102	2532.793089	17.849037	-0.069668	2.747501
368.294415	2524.795422	17.854042	-0.069668	2.743327
367.990298	2516.850155	17.859047	-0.069606	2.739153
368.117785	2508.878714	17.864051	-0.069625	2.734985
368.362962	2500.807737	17.869056	-0.069665	2.730767
368.160643	2492.902473	17.874061	-0.069622	2.726601
368.194348	2484.921193	17.879066	-0.069623	2.722403
368.276110	2476.944647	17.884071	-0.069633	2.718205
368.190504	2469.009397	17.889075	-0.069612	2.714011
368.040234	2461.008690	17.894080	-0.069579	2.709772
367.843450	2453.108694	17.899085	-0.069537	2.705577
367.924942	2445.097383	17.904090	-0.069547	2.701334
367.514072	2437.165329	17.909095	-0.069465	2.697094
367.498553	2429.190954	17.914099	-0.069457	2.692851
367.298244	2421.197756	17.919104	-0.069414	2.688579
367.438678	2413.202186	17.924109	-0.069435	2.684322
367.004332	2405.300995	17.929114	-0.069349	2.680070
367.277145	2397.276092	17.934119	-0.069395	2.675792
367.440855	2389.284775	17.939123	-0.069420	2.671517
367.121809	2381.293285	17.944128	-0.069355	2.667204
366.953917	2373.357241	17.949133	-0.069319	2.662924
366.717624	2365.405407	17.954138	-0.069270	2.658624
367.054670	2357.352053	17.959143	-0.069327	2.654300
367.089781	2349.373380	17.964147	-0.069328	2.649989
367.274774	2341.379359	17.969152	-0.069357	2.645673
367.518645	2333.419748	17.974157	-0.069398	2.641373
367.266841	2325.505651	17.979162	-0.069346	2.637057
367.185401	2317.547971	17.984167	-0.069325	2.632721
366.830758	2309.614501	17.989171	-0.069254	2.628373
366.324292	2301.689549	17.994176	-0.069154	2.624013
366.857266	2293.608838	17.999181	-0.069248	2.619630
366.704292	2285.684495	18.004186	-0.069215	2.615279
366.763881	2277.665827	18.009191	-0.069220	2.610884
366.155261	2269.802774	18.014195	-0.069102	2.606520
366.390499	2261.764949	18.019200	-0.069140	2.602112
366.414886	2253.810929	18.024205	-0.069140	2.597727
366.136094	2245.853125	18.029210	-0.069083	2.593312
366.488083	2237.699605	18.034215	-0.069143	2.588825
366.976188	2229.676480	18.039219	-0.069228	2.584412
365.981673	2221.923833	18.044224	-0.069038	2.580038
366.177192	2213.908922	18.049229	-0.069069	2.575594
366.240132	2205.898496	18.054234	-0.069076	2.571135
366.005732	2197.982154	18.059239	-0.069027	2.566700
365.633979	2190.101842	18.064243	-0.068953	2.562268
365.611583	2182.108457	18.069248	-0.068943	2.557790
366.369933	2174.007805	18.074253	-0.069079	2.553299
366.126722	2166.078858	18.079258	-0.069028	2.548826
365.698368	2158.172149	18.084263	-0.068944	2.544343
366.182947	2150.145781	18.089267	-0.069028	2.539851
366.119943	2142.175150	18.094272	-0.069011	2.535343
365.992866	2134.269673	18.099277	-0.068983	2.530859
366.252511	2126.219579	18.104282	-0.069026	2.526314
366.036256	2118.343447	18.109287	-0.068980	2.521824
365.670861	2110.443166	18.114291	-0.068907	2.517301
365.317500	2102.480241	18.119296	-0.068836	2.512736
365.578889	2094.433286	18.124301	-0.068879	2.508159
365.706783	2086.435332	18.129306	-0.068898	2.503593
365.186675	2078.583110	18.134311	-0.068796	2.499053
365.700800	2070.528669	18.139315	-0.068886	2.494466
365.633695	2062.569575	18.144320	-0.068869	2.489882
365.679536	2054.601510	18.149325	-0.068872	2.485293
365.600952	2046.650878	18.154330	-0.068852	2.480696
365.435542	2038.731777	18.159335	-0.068816	2.476102
365.253047	2030.798765	18.164339	-0.068777	2.471490
365.387021	2022.762867	18.169344	-0.068797	2.466834
365.738473	2014.755287	18.174349	-0.068857	2.462202
365.156950	2006.904860	18.179354	-0.068743	2.457582
365.049672	1998.941358	18.184359	-0.068718	2.452923
365.052340	1990.980400	18.189363	-0.068713	2.448265
364.631798	1983.049820	18.194368	-0.068630	2.443583
365.052153	1975.034536	18.199373	-0.068703	2.438908
364.833748	1967.084042	18.204378	-0.068657	2.434213
364.814104	1959.075553	18.209383	-0.068648	2.429489
364.905529	1951.108001	18.214387	-0.068660	2.424790
365.105906	1943.097323	18.219392	-0.068692	2.420064
365.304378	1935.136855	18.224397	-0.068724	2.415359
365.064585	1927.204357	18.229402	-0.068674	2.410626
364.960769	1919.277257	18.234407	-0.068649	2.405898
364.212735	1911.470105	18.239411	-0.068505	2.401181
364.648376	1903.391412	18.244416	-0.068581	2.396387
364.418271	1895.475282	18.249421	-0.068532	2.391627
364.135259	1887.525781	18.254426	-0.068475	2.386833
364.489926	1879.497722	18.259431	-0.068535	2.382034
363.798602	1871.678440	18.264435	-0.068401	2.377266
364.280399	1863.586145	18.269440	-0.068486	2.372420
364.384566	1855.623256	18.274445	-0.068500	2.367610
363.960326	1847.746241	18.279450	-0.068416	2.362800
364.133393	1839.746243	18.284455	-0.068443	2.357955
364.458457	1831.762923	18.289459	-0.068498	2.353122
364.093866	1823.827472	18.294464	-0.068425	2.348251
364.153519	1815.865211	18.299469	-0.068431	2.343389
363.946898	1807.938947	18.304474	-0.068387	2.338517
363.925869	1799.981873	18.309479	-0.068378	2.333631
363.899955	1792.020585	18.314483	-0.068368	2.328731
363.945445	1784.033136	18.319488	-0.068371	2.323812
364.055913	1776.096307	18.324493	-0.068387	2.318918
363.691253	1768.225295	18.329498	-0.068313	2.314015
363.944216	1760.190461	18.334503	-0.068355	2.309052
363.464606	1752.317283	18.339507	-0.068261	2.304117
363.507294	1744.351940	18.344512	-0.068263	2.299158
363.520444	1736.397581	18.349517	-0.068261	2.294193
363.077387	1728.492632	18.354522	-0.068173	2.289208
362.897474	1720.532930	18.359527	-0.068134	2.284201
363.277949	1712.541584	18.364531	-0.068200	2.279212
363.580376	1704.513934	18.369536	-0.068251	2.274182
363.205207	1696.606482	18.374541	-0.068176	2.269158
363.491116	1688.582552	18.379546	-0.068224	2.264107
363.525146	1680.643176	18.384551	-0.068225	2.259076
363.504540	1672.722454	18.389555	-0.068216	2.254041
363.025771	1664.848265	18.394560	-0.068122	2.248983
363.003564	1656.891029	18.399565	-0.068112	2.243902
363.263675	1648.909538	18.404570	-0.068155	2.238819
363.417992	1640.937492	18.409575	-0.068179	2.233721
363.006216	1633.077213	18.414579	-0.068097	2.228632
362.859404	1625.106595	18.419584	-0.068064	2.223484
362.399742	1617.252497	18.424589	-0.067974	2.218371
362.483871	1609.266057	18.429594	-0.067984	2.213210
362.270109	1601.321549	18.434599	-0.067939	2.208036
361.961721	1593.413753	18.439603	-0.067876	2.202866
362.126175	1585.419398	18.444608	-0.067902	2.197671
361.857577	1577.528216	18.449613	-0.067847	2.192491
361.847770	1569.553587	18.454618	-0.067840	2.187268
362.148251	1561.520326	18.459623	-0.067890	2.182023
362.418963	1553.556833	18.464627	-0.067935	2.176808
361.902524	1545.696928	18.469632	-0.067834	2.171575
362.594198	1537.618769	18.474637	-0.067958	2.166300
362.292288	1529.746456	18.479642	-0.067896	2.161053
362.386262	1521.813953	18.484647	-0.067908	2.155792
362.331586	1513.919255	18.489651	-0.067893	2.150529
361.697927	1506.054262	18.494656	-0.067770	2.145217
361.581593	1498.118210	18.499661	-0.067743	2.139894
361.623338	1490.160370	18.504666	-0.067746	2.134558
361.723306	1482.184541	18.509671	-0.067759	2.129203
361.387814	1474.310794	18.514675	-0.067691	2.123860
361.934956	1466.246831	18.519680	-0.067788	2.118462
361.745294	1458.355279	18.524685	-0.067747	2.113094
362.170652	1450.310250	18.529690	-0.067821	2.107669
362.083966	1442.406654	18.534695	-0.067800	2.102276
361.857190	1434.549922	18.539699	-0.067753	2.096887
361.841512	1426.598332	18.544704	-0.067744	2.091441
361.528879	1418.720971	18.549709	-0.067681	2.086001
361.470088	1410.789260	18.554714	-0.067665	2.080535
361.516517	1402.847671	18.559719	-0.067668	2.075058
361.658948	1394.910456	18.564723	-0.067690	2.069580
361.236207	1387.009579	18.569728	-0.067606	2.064055
361.369958	1379.074687	18.574733	-0.067625	2.058548
360.996988	1371.205438	18.579738	-0.067551	2.053020
360.877318	1363.256853	18.584743	-0.067523	2.047448
360.511946	1355.387300	18.589747	-0.067450	2.041890
360.757460	1347.384791	18.594752	-0.067491	2.036287
361.010021	1339.412551	18.599757	-0.067532	2.030691
360.706895	1331.528404	18.604762	-0.067471	2.025084
360.444227	1323.634597	18.609767	-0.067417	2.019458
360.970445	1315.620308	18.614771	-0.067509	2.013814
360.775629	1307.704309	18.619776	-0.067468	2.008148
360.841902	1299.781979	18.624781	-0.067475	2.002489
361.261143	1291.807888	18.629786	-0.067548	1.996815
361.168116	1283.904733	18.634791	-0.067525	1.991121
360.636369	1276.084541	18.639795	-0.067421	1.985423
360.634611	1268.145275	18.644800	-0.067416	1.979679
360.760999	1260.225956	18.649805	-0.067434	1.973948
360.379076	1252.362194	18.654810	-0.067358	1.968184
359.950759	1244.482361	18.659815	-0.067273	1.962387
360.265043	1236.517546	18.664819	-0.067326	1.956592
360.135698	1228.601159	18.669824	-0.067297	1.950766
360.485184	1220.586412	18.674829	-0.067356	1.944904
360.498895	1212.688991	18.679834	-0.067354	1.939073
360.367184	1204.782533	18.684839	-0.067324	1.933202
360.297328	1196.883269	18.689843	-0.067306	1.927325
360.050335	1188.994370	18.694848	-0.067255	1.921417
360.116472	1181.081192	18.699853	-0.067262	1.915509
360.151236	1173.156570	18.704858	-0.067263	1.909571
360.289562	1165.202054	18.709863	-0.067284	1.903603
360.220850	1157.327790	18.714867	-0.067266	1.897653
360.164180	1149.418966	18.719872	-0.067250	1.891660
360.071621	1141.516477	18.724877	-0.067227	1.885648
360.243633	1133.600870	18.729882	-0.067254	1.879638
360.393925	1125.663550	18.734887	-0.067277	1.873589
360.123344	1117.822232	18.739891	-0.067222	1.867545
360.084882	1109.898178	18.744896	-0.067209	1.861445
360.024673	1102.027259	18.749901	-0.067193	1.855364
359.661219	1094.171202	18.754906	-0.067120	1.849238
359.127232	1086.339620	18.759911	-0.067015	1.843090
359.612167	1078.353830	18.764915	-0.067100	1.836923
359.396773	1070.478899	18.769920	-0.067055	1.830738
359.433623	1062.542130	18.774925	-0.067057	1.824514
359.552240	1054.642481	18.779930	-0.067074	1.818308
359.335143	1046.775086	18.784935	-0.067028	1.812065
359.052790	1038.921293	18.789939	-0.066970	1.805803
359.246423	1030.981318	18.794944	-0.067001	1.799510
358.957081	1023.140831	18.799949	-0.066942	1.793214
358.506347	1015.281063	18.804954	-0.066853	1.786860
358.614904	1007.336334	18.809959	-0.066868	1.780485
358.497590	999.478311	18.814963	-0.066841	1.774129
358.290886	991.598021	18.819968	-0.066797	1.767720
358.149491	983.711323	18.824973	-0.066766	1.761291
358.325932	975.787895	18.829978	-0.066793	1.754850
358.316437	967.888806	18.834983	-0.066786	1.748380
358.341628	960.012140	18.839987	-0.066786	1.741910
357.890128	952.191404	18.844992	-0.066697	1.735399
357.821671	944.311730	18.849997	-0.066679	1.728865
357.642861	936.463492	18.855002	-0.066640	1.722318
357.325028	928.627182	18.860007	-0.066576	1.715738
357.020526	920.791744	18.865011	-0.066514	1.709135
356.925324	912.881117	18.870016	-0.066491	1.702470
357.424759	904.884135	18.875021	-0.066579	1.695786
357.169882	897.062468	18.880026	-0.066526	1.689123
357.063306	889.197798	18.885031	-0.066501	1.682417
356.560521	881.448804	18.890035	-0.066403	1.675729
356.420590	873.555429	18.895040	-0.066371	1.668939
356.905529	865.568352	18.900045	-0.066457	1.662127
356.781349	857.741000	18.905050	-0.066428	1.655341
356.564772	849.897046	18.910055	-0.066383	1.648500
356.524462	842.036921	18.915059	-0.066370	1.641641
356.249137	834.226406	18.920064	-0.066314	1.634763
356.509262	826.271098	18.925069	-0.066357	1.627805
356.906023	818.334956	18.930074	-0.066426	1.620853
356.710285	810.532590	18.935079	-0.066384	1.613905
356.665081	802.701114	18.940083	-0.066370	1.606923
356.085166	794.945131	18.945088	-0.066257	1.599901
356.656168	787.002780	18.950093	-0.066358	1.592847
356.605181	779.154002	18.955098	-0.066344	1.585756
356.698196	771.300905	18.960103	-0.066356	1.578650
356.802613	763.468659	18.965107	-0.066370	1.571532
356.534866	755.670997	18.970112	-0.066315	1.564359
356.340417	747.889983	18.975117	-0.066274	1.557179
356.150593	740.082172	18.980122	-0.066233	1.549941
356.293793	732.202301	18.985127	-0.066255	1.542653
356.036462	724.415370	18.990131	-0.066202	1.535356
355.897458	716.601668	18.995136	-0.066171	1.528017
355.972472	708.741705	19.000141	-0.066180	1.520632
356.083310	700.916205	19.005146	-0.066195	1.513249
355.663002	693.158267	19.010151	-0.066112	1.505812
355.574385	685.372246	19.015155	-0.066090	1.498362
355.404336	677.558633	19.020160	-0.066053	1.490836
354.761623	669.855137	19.025165	-0.065929	1.483304
355.194871	661.943530	19.030170	-0.066004	1.475702
355.094395	654.095229	19.035175	-0.065980	1.468036
355.393496	646.239196	19.040179	-0.066031	1.460388
355.256661	638.456759	19.045184	-0.066000	1.452701
355.683143	630.577080	19.050189	-0.066074	1.444969
355.206137	622.910452	19.055194	-0.065981	1.437259
355.118736	615.121190	19.060199	-0.065959	1.429449
355.408969	607.276424	19.065203	-0.066008	1.421603
355.305302	599.508802	19.070208	-0.065984	1.413726
355.508218	591.686064	19.075213	-0.066016	1.405800
355.636066	583.918299	19.080218	-0.066035	1.397873
355.125536	576.234015	19.085223	-0.065935	1.389878
354.523100	568.572499	19.090227	-0.065818	1.381843
354.432657	560.791843	19.095232	-0.065796	1.373726
354.359770	553.017527	19.100237	-0.065777	1.365571
354.599992	545.217391	19.105242	-0.065817	1.357394
354.744372	537.411974	19.110247	-0.065838	1.349146
354.876533	529.647087	19.115251	-0.065858	1.340888
354.850575	521.923056	19.120256	-0.065848	1.332594
354.820975	514.183914	19.125261	-0.065837	1.324231
354.261113	506.567189	19.130266	-0.065728	1.315851
354.324327	498.717851	19.135271	-0.065735	1.307277
354.123551	491.030235	19.140275	-0.065692	1.298776
354.006955	483.303786	19.145280	-0.065665	1.290192
353.653693	475.642109	19.150285	-0.065595	1.281578
353.632415	467.935662	19.155290	-0.065586	1.272918
354.045602	460.126771	19.160295	-0.065657	1.264166
354.251464	452.390369	19.165299	-0.065691	1.255396
353.714234	444.797045	19.170304	-0.065586	1.246584
354.158966	437.032407	19.175309	-0.065663	1.237703
353.971515	429.384989	19.180314	-0.065623	1.228770
353.297322	421.821053	19.185319	-0.065493	1.219772
353.250295	414.150848	19.190323	-0.065479	1.210708
353.285708	406.460029	19.195328	-0.065481	1.201567
353.946277	398.676281	19.200333	-0.065599	1.192373
353.515786	391.110882	19.205338	-0.065513	1.183147
353.376119	383.486510	19.210343	-0.065482	1.173836
353.465394	375.833473	19.215347	-0.065494	1.164464
353.478337	368.207706	19.220352	-0.065491	1.155033
353.470368	360.553787	19.225357	-0.065485	1.145486
353.558753	352.923343	19.230362	-0.065496	1.135908
352.779519	345.452385	19.235367	-0.065346	1.126262
353.211173	337.778967	19.240371	-0.065422	1.116540
353.050871	330.212025	19.245376	-0.065387	1.106739
352.927786	322.647812	19.250381	-0.065359	1.096862
353.191694	315.026340	19.255386	-0.065403	1.086908
352.829587	307.541431	19.260391	-0.065331	1.076899
352.873979	299.979759	19.265395	-0.065334	1.066788
352.448306	292.504999	19.270400	-0.065250	1.056588
352.240034	284.997745	19.275405	-0.065206	1.046295
352.807673	277.372522	19.280410	-0.065307	1.035923
352.567044	269.903516	19.285415	-0.065257	1.025468
352.121370	262.506619	19.290419	-0.065169	1.014957
351.844874	255.052937	19.295424	-0.065113	1.004297
351.587017	247.618570	19.300429	-0.065060	0.993555
351.144920	240.210143	19.305434	-0.064973	0.982686
351.078933	232.747369	19.310439	-0.064955	0.971712
351.447302	225.236076	19.315443	-0.065019	0.960654
351.219530	217.850981	19.320448	-0.064972	0.949500
351.889258	210.317313	19.325453	-0.065092	0.938226
351.082156	203.091433	19.330458	-0.064937	0.926892
350.515421	195.836479	19.335463	-0.064826	0.915437
351.170425	188.347563	19.340467	-0.064943	0.903806
351.039730	181.034046	19.345472	-0.064914	0.892084
351.118879	173.706933	19.350477	-0.064924	0.880243
350.878823	166.471058	19.355482	-0.064875	0.868299
351.187371	159.142073	19.360487	-0.064927	0.856194
350.368888	152.068980	19.365491	-0.064770	0.844012
349.922706	144.914611	19.370496	-0.064682	0.831625
349.744483	137.722109	19.375501	-0.064644	0.819067
349.522883	130.579940	19.380506	-0.064599	0.806389
349.088871	123.496341	19.385511	-0.064513	0.793545
348.913967	116.403433	19.390515	-0.064476	0.780558
348.177285	109.425012	19.395520	-0.064334	0.767378
346.729369	102.611640	19.400525	-0.064060	0.754041
345.920262	95.681493	19.405530	-0.063905	0.740457
345.220377	88.766263	19.410535	-0.063770	0.726686
344.265852	81.953592	19.415539	-0.063588	0.712764
343.676350	75.267506	19.420544	-0.063473	0.698957