Mon Apr 19 09:03:07 2021

Number of Points = 3632
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
2.275499	0.166890	0.000000	0.000169	0.308920

2.127225	0.192740	0.005005	0.000196	0.308915
2.397613	0.142086	0.010010	0.000146	0.308908
2.157022	0.188504	0.015014	0.000191	0.308920
2.292720	0.159797	0.020019	0.000166	0.308901
2.247448	0.171406	0.025024	0.000174	0.308917
2.515458	0.119030	0.030029	0.000124	0.308899
2.351414	0.150078	0.035034	0.000155	0.308905
2.388835	0.143726	0.040038	0.000148	0.308907
2.271722	0.164497	0.045043	0.000170	0.308904
2.479371	0.129066	0.050048	0.000131	0.308915
2.166298	0.186242	0.055053	0.000190	0.308916
2.451280	0.133336	0.060058	0.000137	0.308910
2.351216	0.153996	0.065062	0.000155	0.308922
2.281074	0.145448	0.070067	0.000168	0.308822
1.851472	0.181838	0.075072	0.000248	0.308626
2.129412	0.127269	0.080077	0.000197	0.308607
1.927014	0.165568	0.085082	0.000234	0.308614
2.130037	0.128811	0.090086	0.000197	0.308615
2.144188	0.124039	0.095091	0.000194	0.308604
2.498483	0.060305	0.100096	0.000128	0.308607
2.453674	0.067058	0.105101	0.000137	0.308600
2.598671	0.040269	0.110106	0.000110	0.308598
2.355631	0.086772	0.115110	0.000155	0.308609
2.300890	0.079358	0.120115	0.000165	0.308527
2.004316	0.084184	0.125120	0.000220	0.308297
2.147626	0.056604	0.130125	0.000194	0.308289
2.442801	0.001324	0.135130	0.000139	0.308281
2.491240	-0.007289	0.140134	0.000130	0.308282
2.458780	-0.003306	0.145139	0.000136	0.308273
2.347836	0.002749	0.150144	0.000157	0.308206
2.189579	-0.012069	0.155149	0.000186	0.308002
2.094769	0.006417	0.160154	0.000204	0.308007
2.528929	-0.074227	0.165158	0.000123	0.307999
2.089026	0.006583	0.170163	0.000205	0.308003
2.375351	-0.082168	0.175168	0.000152	0.307830
2.346287	-0.114515	0.180173	0.000157	0.307653
2.065308	-0.061586	0.185178	0.000210	0.307661
2.142755	-0.073851	0.190182	0.000195	0.307670
1.998437	-0.074147	0.195187	0.000222	0.307545
2.151493	-0.142908	0.200192	0.000194	0.307352
2.381344	-0.187355	0.205197	0.000151	0.307339
2.560795	-0.220486	0.210202	0.000118	0.307336
2.667041	-0.294820	0.215206	0.000098	0.307077
2.580886	-0.296054	0.220211	0.000114	0.306997
2.527133	-0.282369	0.225216	0.000124	0.307015
2.227806	-0.271720	0.230221	0.000180	0.306809
2.453768	-0.331665	0.235226	0.000138	0.306720
2.383389	-0.317101	0.240230	0.000151	0.306728
2.305983	-0.357221	0.245235	0.000166	0.306472
2.206849	-0.355344	0.250240	0.000184	0.306396
2.373866	-0.387706	0.255245	0.000153	0.306386
2.344646	-0.440933	0.260250	0.000159	0.306109
2.484616	-0.472164	0.265254	0.000133	0.306082
1.742398	-0.350369	0.270259	0.000271	0.306020
2.163510	-0.479449	0.275264	0.000192	0.305771
2.312948	-0.507888	0.280269	0.000165	0.305764
2.193237	-0.523325	0.285274	0.000187	0.305588
2.645083	-0.623380	0.290278	0.000103	0.305503
2.726255	-0.667040	0.295283	0.000088	0.305366
2.721072	-0.710898	0.300288	0.000089	0.305153
2.890167	-0.758633	0.305293	0.000058	0.305072
2.433225	-0.725720	0.310298	0.000143	0.304834
2.309739	-0.706589	0.315302	0.000166	0.304819
2.527735	-0.812910	0.320307	0.000125	0.304502
2.641411	-0.833836	0.325312	0.000104	0.304500
2.654477	-0.895105	0.330317	0.000102	0.304220
2.218670	-0.816797	0.335322	0.000183	0.304215
2.522595	-0.941507	0.340326	0.000126	0.303885
2.287327	-0.903617	0.345331	0.000170	0.303861
2.110293	-0.928273	0.350336	0.000203	0.303590
2.185061	-0.951777	0.355341	0.000189	0.303543
2.257309	-1.024195	0.360346	0.000176	0.303260
2.269746	-1.038975	0.365350	0.000174	0.303200
2.469976	-1.125513	0.370355	0.000137	0.302960
2.420446	-1.147137	0.375360	0.000146	0.302814
2.215652	-1.148172	0.380365	0.000184	0.302631
1.831186	-1.120228	0.385370	0.000256	0.302430
2.035744	-1.178538	0.390374	0.000218	0.302329
2.116028	-1.254758	0.395379	0.000203	0.302033
1.987764	-1.245880	0.400384	0.000227	0.301964
1.868122	-1.275449	0.405389	0.000249	0.301718
2.243584	-1.378291	0.410394	0.000179	0.301552
2.164735	-1.400858	0.415398	0.000194	0.301374
1.877594	-1.402457	0.420403	0.000248	0.301116
1.478934	-1.344063	0.425408	0.000322	0.301048
1.612220	-1.426680	0.430413	0.000297	0.300767
1.067318	-1.347146	0.435418	0.000399	0.300673
1.105284	-1.379935	0.440422	0.000392	0.300548
1.578759	-1.525517	0.445427	0.000303	0.300261
1.621504	-1.559642	0.450432	0.000296	0.300134
1.858507	-1.660268	0.455437	0.000252	0.299856
1.558897	-1.647307	0.460442	0.000307	0.299656
1.471126	-1.660017	0.465446	0.000324	0.299517
1.657208	-1.750161	0.470451	0.000289	0.299245
1.958781	-1.848462	0.475456	0.000233	0.299034
1.654801	-1.829255	0.480461	0.000290	0.298860
1.623154	-1.875929	0.485466	0.000296	0.298605
1.453843	-1.893092	0.490470	0.000327	0.298373
1.548611	-1.947654	0.495475	0.000310	0.298192
1.766636	-2.028778	0.500480	0.000269	0.297990
1.470628	-2.038000	0.505485	0.000324	0.297684
1.304673	-2.048435	0.510490	0.000355	0.297486
1.460826	-2.116781	0.515494	0.000326	0.297291
0.903941	-2.069727	0.520499	0.000430	0.297027
0.824990	-2.096906	0.525504	0.000445	0.296825
0.984327	-2.165537	0.530509	0.000415	0.296631
1.351237	-2.281919	0.535514	0.000347	0.296388
1.205881	-2.317095	0.540518	0.000374	0.296087
0.721779	-2.272969	0.545523	0.000464	0.295873
0.612914	-2.288416	0.550528	0.000485	0.295700
0.685015	-2.337658	0.555533	0.000471	0.295523
0.645031	-2.399423	0.560538	0.000479	0.295185
0.115958	-2.343809	0.565542	0.000577	0.294986
0.071838	-2.378701	0.570547	0.000586	0.294775
0.213037	-2.452326	0.575552	0.000560	0.294539
0.055328	-2.479575	0.580557	0.000589	0.294264
0.167891	-2.545358	0.585562	0.000568	0.294041
0.044711	-2.568741	0.590566	0.000591	0.293815
-0.006656	-2.608396	0.595571	0.000601	0.293574
-0.576820	-2.562186	0.600576	0.000707	0.293290
-1.100865	-2.504167	0.605581	0.000804	0.293106
-1.323501	-2.501125	0.610586	0.000846	0.292921
-2.042161	-2.420348	0.615590	0.000980	0.292675
-2.627748	-2.361592	0.620595	0.001089	0.292439
-2.168691	-2.476428	0.625600	0.001003	0.292283
-2.747864	-2.421923	0.630605	0.001111	0.292031
-2.984503	-2.419186	0.635610	0.001155	0.291831
-2.970961	-2.448089	0.640614	0.001153	0.291700
-3.491999	-2.414511	0.645619	0.001250	0.291396
-3.246414	-2.491364	0.650624	0.001204	0.291236
-3.709187	-2.435333	0.655629	0.001291	0.291096
-3.759951	-2.488006	0.660634	0.001300	0.290788
-3.915207	-2.480820	0.665638	0.001329	0.290683
-4.636718	-2.380743	0.670643	0.001463	0.290528
-4.399494	-2.471580	0.675648	0.001419	0.290290
-4.821335	-2.420439	0.680653	0.001498	0.290163
-4.994101	-2.453504	0.685658	0.001530	0.289841
-5.203034	-2.434173	0.690662	0.001569	0.289748
-5.683017	-2.391841	0.695667	0.001658	0.289523
-5.865170	-2.390889	0.700672	0.001692	0.289362
-6.258671	-2.343181	0.705677	0.001766	0.289243
-6.363760	-2.374651	0.710682	0.001785	0.288989
-6.324252	-2.398831	0.715686	0.001778	0.288904
-7.026564	-2.325521	0.720691	0.001909	0.288631
-6.941712	-2.346682	0.725696	0.001893	0.288602
-7.734365	-2.264924	0.730701	0.002041	0.288289
-7.740796	-2.268734	0.735706	0.002042	0.288264
-7.685750	-2.329371	0.740710	0.002032	0.288009
-7.561138	-2.360687	0.745715	0.002009	0.287966
-7.388965	-2.459046	0.750720	0.001977	0.287628
-7.814544	-2.387641	0.755725	0.002056	0.287598
-8.489756	-2.319265	0.760730	0.002182	0.287324
-8.251582	-2.367305	0.765734	0.002137	0.287300
-8.724457	-2.342207	0.770739	0.002225	0.286993
-8.985368	-2.292869	0.775744	0.002274	0.287002
-9.122300	-2.326272	0.780749	0.002300	0.286708
-9.589045	-2.239577	0.785754	0.002386	0.286717
-9.302741	-2.350337	0.790758	0.002333	0.286420
-9.869793	-2.257516	0.795763	0.002439	0.286368
-9.733033	-2.327937	0.800768	0.002413	0.286138
-9.718563	-2.345209	0.805773	0.002411	0.286063
-9.553270	-2.418244	0.810778	0.002380	0.285846
-10.280368	-2.304934	0.815782	0.002515	0.285750
-10.366701	-2.317033	0.820787	0.002532	0.285609
-10.291405	-2.354652	0.825792	0.002518	0.285487
-10.418277	-2.358178	0.830797	0.002541	0.285352
-11.078397	-2.279356	0.835802	0.002664	0.285143
-10.986228	-2.304381	0.840806	0.002647	0.285101
-11.047389	-2.348753	0.845811	0.002659	0.284819
-11.115046	-2.335231	0.850816	0.002671	0.284825
-11.390412	-2.347789	0.855821	0.002723	0.284506
-11.970883	-2.242348	0.860826	0.002831	0.284505
-11.914973	-2.291655	0.865830	0.002820	0.284306
-12.374407	-2.227506	0.870835	0.002906	0.284207
-11.859838	-2.343742	0.875840	0.002810	0.284091
-12.371278	-2.293977	0.880845	0.002905	0.283871
-12.572177	-2.260832	0.885850	0.002943	0.283853
-12.407105	-2.347483	0.890854	0.002912	0.283564
-12.796967	-2.276756	0.895859	0.002985	0.283563
-12.920916	-2.299561	0.900864	0.003008	0.283331
-13.554516	-2.198331	0.905869	0.003126	0.283260
-13.284177	-2.266858	0.910874	0.003076	0.283160
-13.651455	-2.239397	0.915878	0.003144	0.282959
-13.716524	-2.228275	0.920883	0.003156	0.282955
-13.636037	-2.296962	0.925888	0.003141	0.282679
-14.080134	-2.228641	0.930893	0.003224	0.282615
-14.528562	-2.167207	0.935898	0.003307	0.282511
-14.371621	-2.236300	0.940902	0.003278	0.282303
-14.513312	-2.210487	0.945907	0.003305	0.282303
-14.733220	-2.217997	0.950912	0.003346	0.282060
-15.136230	-2.159352	0.955917	0.003421	0.281984
-14.828116	-2.225191	0.960922	0.003363	0.281934
-15.292585	-2.186139	0.965926	0.003450	0.281700
-15.587866	-2.133725	0.970931	0.003505	0.281693
-15.628144	-2.152655	0.975936	0.003512	0.281558
-15.948329	-2.131243	0.980941	0.003572	0.281369
-15.779801	-2.164975	0.985946	0.003541	0.281353
-15.440623	-2.269663	0.990950	0.003478	0.281131
-16.211489	-2.144332	0.995955	0.003621	0.281054
-16.381411	-2.119761	1.000960	0.003653	0.281022
-16.467819	-2.158982	1.005965	0.003669	0.280738
-16.991316	-2.060910	1.010970	0.003767	0.280753
-17.032832	-2.065049	1.015974	0.003774	0.280692
-17.209964	-2.068783	1.020979	0.003807	0.280507
-17.003580	-2.104342	1.025984	0.003769	0.280517
-17.011896	-2.130780	1.030989	0.003771	0.280372
-17.727602	-2.040660	1.035994	0.003904	0.280165
-17.329225	-2.111079	1.040998	0.003830	0.280176
-17.735811	-2.073171	1.046003	0.003906	0.279989
-17.917782	-2.066082	1.051008	0.003939	0.279855
-17.799992	-2.087144	1.056013	0.003918	0.279856
-18.108562	-2.077782	1.061018	0.003975	0.279614
-17.972859	-2.119203	1.066022	0.003950	0.279527
-18.367169	-2.048120	1.071027	0.004023	0.279524
-18.038142	-2.158859	1.076032	0.003962	0.279260
-18.295627	-2.115410	1.081037	0.004010	0.279242
-18.980607	-1.999488	1.086042	0.004138	0.279197
-19.303595	-1.993133	1.091046	0.004198	0.278925
-19.115753	-2.028548	1.096051	0.004163	0.278918
-18.915200	-2.078336	1.101056	0.004126	0.278849
-20.231456	-1.881661	1.106061	0.004371	0.278627
-19.693411	-1.983508	1.111066	0.004271	0.278606
-19.381408	-2.045111	1.116070	0.004213	0.278581
-20.307562	-1.931618	1.121075	0.004385	0.278295
-20.008262	-1.986649	1.126080	0.004329	0.278291
-19.750443	-2.037253	1.131085	0.004281	0.278272
-20.713670	-1.913645	1.136090	0.004461	0.278003
-20.192427	-2.009135	1.141094	0.004364	0.277999
-20.242183	-2.001704	1.146099	0.004373	0.277991
-20.179322	-2.079655	1.151104	0.004361	0.277644
-20.503000	-2.020151	1.156109	0.004422	0.277647
-20.471055	-2.037509	1.161114	0.004416	0.277587
-20.528651	-2.072999	1.166118	0.004427	0.277347
-20.772063	-2.032753	1.171123	0.004472	0.277325
-20.781355	-2.055318	1.176128	0.004474	0.277198
-21.024217	-2.044778	1.181133	0.004519	0.277023
-21.025208	-2.047804	1.186138	0.004519	0.277006
-21.601812	-1.971099	1.191142	0.004627	0.276858
-21.549927	-2.006210	1.196147	0.004617	0.276724
-21.266208	-2.057887	1.201152	0.004564	0.276723
-21.327387	-2.095272	1.206157	0.004576	0.276469
-21.749164	-2.035816	1.211162	0.004654	0.276378
-21.809401	-2.020498	1.216166	0.004665	0.276401
-22.122822	-2.024761	1.221171	0.004724	0.276080
-22.579175	-1.939137	1.226176	0.004809	0.276093
-22.862150	-1.884613	1.231181	0.004862	0.276109
-22.599339	-1.995583	1.236186	0.004813	0.275777
-23.101832	-1.900931	1.241190	0.004906	0.275794
-23.179995	-1.889491	1.246195	0.004921	0.275780
-23.160097	-1.932487	1.251200	0.004917	0.275573
-23.112377	-1.948929	1.256205	0.004908	0.275532
-23.276824	-1.920559	1.261210	0.004939	0.275523
-22.488296	-2.123693	1.266214	0.004792	0.275209
-23.457314	-1.952827	1.271219	0.004973	0.275181
-23.391394	-1.974551	1.276224	0.004961	0.275129
-23.169740	-2.065029	1.281229	0.004919	0.274865
-23.344456	-2.035150	1.286234	0.004952	0.274855
-23.855972	-1.967394	1.291238	0.005047	0.274721
-24.465186	-1.889092	1.296243	0.005161	0.274550
-23.949670	-1.980080	1.301248	0.005065	0.274564
-23.921063	-2.016764	1.306253	0.005059	0.274398
-24.948999	-1.854180	1.311258	0.005251	0.274269
-24.431967	-1.948024	1.316262	0.005155	0.274270
-24.615058	-1.954205	1.321267	0.005189	0.274061
-25.220589	-1.867053	1.326272	0.005302	0.273939
-24.688897	-1.965007	1.331277	0.005203	0.273933
-24.957453	-1.958400	1.336282	0.005253	0.273709
-25.623053	-1.851860	1.341286	0.005377	0.273632
-25.039965	-1.963319	1.346291	0.005268	0.273603
-25.107049	-1.995736	1.351296	0.005281	0.273367
-25.989985	-1.846071	1.356301	0.005445	0.273309
-25.740445	-1.894696	1.361306	0.005399	0.273291
-25.331723	-2.012736	1.366310	0.005323	0.273059
-25.496182	-1.996099	1.371315	0.005353	0.272989
-25.618622	-1.984012	1.376320	0.005376	0.272935
-25.495522	-2.060670	1.381325	0.005353	0.272646
-25.429116	-2.075339	1.386330	0.005341	0.272632
-25.771852	-2.046065	1.391334	0.005405	0.272456
-26.093319	-2.012031	1.396339	0.005465	0.272326
-25.964320	-2.033922	1.401344	0.005441	0.272335
-26.421923	-2.010191	1.406349	0.005526	0.272018
-26.984753	-1.907772	1.411354	0.005631	0.272018
-26.926496	-1.925545	1.416358	0.005620	0.271979
-26.966344	-1.966394	1.421363	0.005627	0.271723
-27.281257	-1.907631	1.426368	0.005686	0.271731
-26.944334	-1.993159	1.431373	0.005623	0.271601
-27.269314	-1.973570	1.436378	0.005684	0.271390
-26.892634	-2.042598	1.441382	0.005614	0.271387
-27.354355	-2.000717	1.446387	0.005700	0.271162
-27.861673	-1.919795	1.451392	0.005794	0.271102
-27.710819	-1.946929	1.456397	0.005766	0.271103
-28.247954	-1.910130	1.461402	0.005866	0.270777
-27.859350	-1.980319	1.466406	0.005794	0.270780
-28.088256	-1.948845	1.471411	0.005837	0.270725
-28.431378	-1.923482	1.476416	0.005901	0.270527
-28.108685	-1.983580	1.481421	0.005841	0.270519
-28.202510	-1.999639	1.486426	0.005858	0.270341
-28.559642	-1.964827	1.491430	0.005925	0.270180
-28.544490	-1.969233	1.496435	0.005922	0.270171
-28.848714	-1.960783	1.501440	0.005979	0.269919
-28.811443	-1.976724	1.506445	0.005972	0.269870
-29.090184	-1.937813	1.511450	0.006024	0.269806
-28.783428	-2.046156	1.516454	0.005967	0.269524
-28.898992	-2.026264	1.521459	0.005988	0.269517
-29.086767	-2.022705	1.526464	0.006023	0.269353
-29.281266	-2.006770	1.531469	0.006060	0.269248
-29.423974	-1.982498	1.536474	0.006086	0.269239
-29.129974	-2.100583	1.541478	0.006031	0.268891
-29.615899	-2.011166	1.546483	0.006122	0.268896
-29.045489	-2.149384	1.551488	0.006016	0.268710
-29.714162	-2.049926	1.556493	0.006140	0.268591
-30.010974	-2.001761	1.561498	0.006196	0.268559
-29.555454	-2.140791	1.566502	0.006111	0.268256
-29.885286	-2.080373	1.571507	0.006172	0.268258
-30.180379	-2.062846	1.576512	0.006227	0.268062
-30.166726	-2.082380	1.581517	0.006225	0.267970
-30.485661	-2.036364	1.586522	0.006284	0.267905
-30.464137	-2.090942	1.591526	0.006280	0.267631
-30.994839	-1.994544	1.596531	0.006379	0.267630
-31.145736	-2.005223	1.601536	0.006407	0.267423
-31.233513	-2.006839	1.606541	0.006424	0.267328
-31.266434	-2.007778	1.611546	0.006430	0.267290
-31.223587	-2.069291	1.616550	0.006422	0.266998
-31.486222	-2.022980	1.621555	0.006471	0.266990
-32.277701	-1.902799	1.626560	0.006618	0.266861
-32.418909	-1.900995	1.631565	0.006645	0.266731
-32.338363	-1.915599	1.636570	0.006630	0.266731
-32.240235	-1.973843	1.641574	0.006611	0.266512
-32.685988	-1.916929	1.646579	0.006694	0.266380
-32.405810	-1.967422	1.651584	0.006642	0.266382
-32.410887	-2.019281	1.656589	0.006643	0.266095
-33.213244	-1.876691	1.661594	0.006793	0.266077
-32.707435	-1.982422	1.666598	0.006699	0.266002
-32.896544	-1.994481	1.671603	0.006734	0.265748
-33.441678	-1.891678	1.676608	0.006835	0.265768
-33.359475	-1.930395	1.681613	0.006820	0.265638
-33.308870	-1.966526	1.686618	0.006811	0.265491
-33.316934	-1.962090	1.691622	0.006812	0.265507
-34.091921	-1.873556	1.696627	0.006957	0.265221
-34.154842	-1.871701	1.701632	0.006968	0.265168
-33.736546	-1.952051	1.706637	0.006891	0.265145
-34.729761	-1.823491	1.711642	0.007075	0.264860
-34.516591	-1.861064	1.716646	0.007036	0.264866
-34.311772	-1.909521	1.721651	0.006998	0.264804
-34.668413	-1.897324	1.726656	0.007064	0.264516
-34.715777	-1.886556	1.731661	0.007073	0.264528
-34.707420	-1.910507	1.736666	0.007072	0.264404
-34.691355	-1.943701	1.741670	0.007069	0.264238
-35.126503	-1.862808	1.746675	0.007150	0.264248
-34.972516	-1.933481	1.751680	0.007121	0.264013
-35.420706	-1.869138	1.756685	0.007205	0.263919
-36.157183	-1.733597	1.761690	0.007342	0.263927
-36.088430	-1.790018	1.766694	0.007329	0.263686
-36.298830	-1.764951	1.771699	0.007368	0.263613
-35.830738	-1.852774	1.776704	0.007281	0.263598
-35.520865	-1.958806	1.781709	0.007223	0.263325
-36.000967	-1.882639	1.786714	0.007313	0.263263
-36.400536	-1.811674	1.791718	0.007387	0.263254
-36.410280	-1.858614	1.796723	0.007389	0.262985
-35.945357	-1.946493	1.801728	0.007303	0.262967
-36.078261	-1.946299	1.806733	0.007327	0.262835
-36.830687	-1.844088	1.811738	0.007468	0.262643
-36.557788	-1.893575	1.816742	0.007417	0.262644
-36.601771	-1.930288	1.821747	0.007425	0.262397
-37.230154	-1.828147	1.826752	0.007542	0.262330
-37.379078	-1.797903	1.831757	0.007570	0.262347
-37.620192	-1.813536	1.836762	0.007615	0.262018
-37.475816	-1.838588	1.841766	0.007588	0.262024
-37.510525	-1.844874	1.846771	0.007594	0.261954
-38.474708	-1.706479	1.851776	0.007774	0.261750
-38.018769	-1.789353	1.856781	0.007689	0.261750
-38.409122	-1.728024	1.861786	0.007762	0.261696
-38.233718	-1.811918	1.866790	0.007729	0.261408
-37.692250	-1.914705	1.871795	0.007629	0.261384
-38.136871	-1.861337	1.876800	0.007711	0.261231
-39.007823	-1.725942	1.881805	0.007873	0.261103
-38.245227	-1.868596	1.886810	0.007732	0.261081
-38.175927	-1.920455	1.891814	0.007719	0.260863
-38.831584	-1.819646	1.896819	0.007841	0.260760
-38.941835	-1.800178	1.901824	0.007861	0.260757
-38.745253	-1.877459	1.906829	0.007825	0.260526
-38.446520	-1.935363	1.911834	0.007769	0.260506
-39.313831	-1.799742	1.916838	0.007931	0.260382
-39.645868	-1.774304	1.921843	0.007993	0.260187
-39.455480	-1.809265	1.926848	0.007957	0.260185
-39.198638	-1.895999	1.931853	0.007910	0.259962
-39.614180	-1.841214	1.936858	0.007987	0.259846
-39.358543	-1.890789	1.941862	0.007939	0.259829
-40.046091	-1.816768	1.946867	0.008067	0.259544
-40.222725	-1.785192	1.951872	0.008100	0.259540
-39.985475	-1.848076	1.956877	0.008056	0.259430
-40.402342	-1.803147	1.961882	0.008134	0.259257
-40.282669	-1.825064	1.966886	0.008112	0.259256
-41.014599	-1.730934	1.971891	0.008248	0.259038
-41.131966	-1.727378	1.976896	0.008270	0.258938
-40.772684	-1.794069	1.981901	0.008203	0.258930
-41.249217	-1.756900	1.986906	0.008292	0.258653
-40.749715	-1.855173	1.991910	0.008199	0.258611
-40.936107	-1.835175	1.996915	0.008234	0.258533
-41.335717	-1.806127	2.001920	0.008308	0.258288

-41.352821	-1.839441	2.011917	0.008311	0.258083
-41.869806	-1.758516	2.021914	0.008408	0.258009
-42.223800	-1.754303	2.031910	0.008474	0.257670
-41.756595	-1.841132	2.041907	0.008387	0.257660
-42.088254	-1.836238	2.051904	0.008449	0.257347
-42.240900	-1.809294	2.061901	0.008477	0.257342
-42.289579	-1.829844	2.071898	0.008486	0.257176
-42.869477	-1.750118	2.081894	0.008594	0.257030
-42.369457	-1.842338	2.091891	0.008501	0.257023
-42.747502	-1.773503	2.101888	0.008572	0.257023
-42.775717	-1.776157	2.111885	0.008577	0.256978
-43.030238	-1.772434	2.121882	0.008625	0.256738
-43.181516	-1.742817	2.131878	0.008653	0.256749
-43.184653	-1.741945	2.141875	0.008654	0.256750
-42.678919	-1.838320	2.151872	0.008560	0.256725
-42.539776	-1.865194	2.161869	0.008534	0.256716
-42.314101	-1.906832	2.171866	0.008492	0.256712
-41.670068	-2.026831	2.181862	0.008372	0.256696
-41.913755	-1.980176	2.191859	0.008417	0.256708
-42.182551	-1.931789	2.201856	0.008468	0.256705
-42.430071	-1.884208	2.211853	0.008514	0.256719
-42.232477	-1.901486	2.221850	0.008477	0.256824
-42.227693	-1.870340	2.231846	0.008476	0.257004
-42.003458	-1.910974	2.241843	0.008435	0.257004
-42.728646	-1.775783	2.251840	0.008570	0.257022
-42.604874	-1.797009	2.261837	0.008547	0.257029
-42.043941	-1.844988	2.271834	0.008442	0.257333
-41.785713	-1.893750	2.281830	0.008394	0.257322
-42.061891	-1.840658	2.291827	0.008446	0.257338
-42.057862	-1.798166	2.301824	0.008445	0.257581
-41.637592	-1.862473	2.311821	0.008367	0.257648
-41.974583	-1.790122	2.321818	0.008430	0.257710
-41.567030	-1.812919	2.331814	0.008354	0.257998
-40.834829	-1.950761	2.341811	0.008218	0.257971
-40.662459	-1.958154	2.351808	0.008186	0.258105
-40.657887	-1.930296	2.361805	0.008185	0.258266
-40.651977	-1.934107	2.371802	0.008184	0.258250
-40.363395	-1.929835	2.381798	0.008130	0.258568
-40.106217	-1.976756	2.391795	0.008083	0.258567
-39.744405	-2.011134	2.401792	0.008015	0.258742
-39.739398	-1.987552	2.411789	0.008015	0.258879
-39.903311	-1.941450	2.421786	0.008045	0.258969
-38.929152	-2.076045	2.431782	0.007864	0.259207
-39.480005	-1.971727	2.441779	0.007967	0.259230
-39.236835	-1.967955	2.451776	0.007921	0.259497
-39.416159	-1.924043	2.461773	0.007955	0.259560
-39.351580	-1.885315	2.471770	0.007943	0.259841
-38.997184	-1.927221	2.481766	0.007877	0.259966
-38.949638	-1.901303	2.491763	0.007868	0.260158
-38.425115	-1.954584	2.501760	0.007771	0.260392
-38.400336	-1.940206	2.511757	0.007766	0.260497
-37.997960	-1.975426	2.521754	0.007691	0.260707
-37.878087	-1.982782	2.531750	0.007669	0.260787
-37.881503	-1.932138	2.541747	0.007670	0.261064
-37.674148	-1.939174	2.551744	0.007631	0.261234
-37.296653	-1.985465	2.561741	0.007561	0.261358
-37.253120	-1.936952	2.571738	0.007553	0.261670
-37.062847	-1.948140	2.581734	0.007518	0.261799
-36.838906	-1.955293	2.591731	0.007476	0.261984
-36.499542	-1.970839	2.601728	0.007413	0.262239
-36.482226	-1.949041	2.611725	0.007410	0.262376
-36.361381	-1.926559	2.621722	0.007387	0.262621
-36.367741	-1.874417	2.631718	0.007389	0.262901
-36.434969	-1.826963	2.641715	0.007401	0.263095
-36.086024	-1.855394	2.651712	0.007336	0.263287
-36.182688	-1.780561	2.661709	0.007354	0.263602
-35.902265	-1.789085	2.671706	0.007302	0.263834
-35.800952	-1.760487	2.681702	0.007283	0.264092
-35.516996	-1.770415	2.691699	0.007231	0.264320
-35.349708	-1.759313	2.701696	0.007200	0.264547
-34.606733	-1.838707	2.711693	0.007061	0.264852
-34.236739	-1.868372	2.721690	0.006993	0.265057
-34.079436	-1.856385	2.731686	0.006963	0.265278
-33.924588	-1.839684	2.741683	0.006935	0.265523
-33.508379	-1.869850	2.751680	0.006857	0.265770
-33.606155	-1.812378	2.761677	0.006876	0.265986
-33.503566	-1.788845	2.771674	0.006856	0.266215
-32.918268	-1.857681	2.781670	0.006748	0.266419
-33.068678	-1.768575	2.791667	0.006776	0.266754
-32.603866	-1.812347	2.801664	0.006689	0.266975
-32.290966	-1.827183	2.811661	0.006631	0.267203
-32.439977	-1.757565	2.821658	0.006659	0.267433
-31.844503	-1.822068	2.831654	0.006548	0.267669
-31.618951	-1.800704	2.841651	0.006506	0.268006
-31.257405	-1.828071	2.851648	0.006439	0.268213
-31.091966	-1.820767	2.861645	0.006408	0.268414
-30.721445	-1.845821	2.871642	0.006339	0.268642
-30.465022	-1.841705	2.881638	0.006292	0.268915
-30.007013	-1.877344	2.891635	0.006207	0.269171
-30.010358	-1.836041	2.901632	0.006207	0.269390
-29.781871	-1.843581	2.911629	0.006165	0.269572
-29.496874	-1.839744	2.921626	0.006112	0.269870
-29.079093	-1.869290	2.931622	0.006034	0.270119
-29.187703	-1.804554	2.941619	0.006054	0.270360
-29.211911	-1.751207	2.951616	0.006059	0.270621
-28.804739	-1.790690	2.961613	0.005983	0.270806
-28.116521	-1.861479	2.971610	0.005855	0.271096
-27.761418	-1.888044	2.981606	0.005789	0.271298
-27.734595	-1.852457	2.991603	0.005784	0.271514
-27.248841	-1.899007	3.001600	0.005694	0.271736
-27.345791	-1.826545	3.011597	0.005712	0.272027
-27.285287	-1.790855	3.021594	0.005701	0.272275
-27.351330	-1.733317	3.031590	0.005713	0.272517
-26.921107	-1.761488	3.041587	0.005633	0.272782
-26.306277	-1.830871	3.051584	0.005519	0.273007
-25.655554	-1.896985	3.061581	0.005398	0.273284
-26.236910	-1.745263	3.071578	0.005506	0.273527
-26.387698	-1.666433	3.081574	0.005534	0.273798
-25.952749	-1.692077	3.091571	0.005453	0.274080
-25.396382	-1.748512	3.101568	0.005350	0.274316
-25.231949	-1.731216	3.111565	0.005319	0.274565
-24.783424	-1.755283	3.121562	0.005236	0.274867
-24.150079	-1.826862	3.131558	0.005118	0.275096
-23.979387	-1.815830	3.141555	0.005086	0.275317
-24.087627	-1.746207	3.151552	0.005107	0.275579
-23.961889	-1.726244	3.161549	0.005083	0.275804
-23.488893	-1.760433	3.171546	0.004995	0.276075
-23.452554	-1.721301	3.181542	0.004989	0.276315
-23.452476	-1.670486	3.191539	0.004989	0.276580
-23.213998	-1.660251	3.201536	0.004944	0.276860
-22.556886	-1.739636	3.211533	0.004822	0.277069
-22.398539	-1.709048	3.221530	0.004793	0.277379
-22.287655	-1.677650	3.231526	0.004772	0.277648
-21.651550	-1.743468	3.241523	0.004654	0.277907
-21.149117	-1.795967	3.251520	0.004560	0.278109
-21.334372	-1.717689	3.261517	0.004595	0.278341
-21.088507	-1.706260	3.271514	0.004549	0.278632
-20.677968	-1.731513	3.281510	0.004473	0.278888
-20.030862	-1.805949	3.291507	0.004352	0.279112
-19.633322	-1.840291	3.301504	0.004279	0.279308
-19.093936	-1.894287	3.311501	0.004178	0.279536
-19.165772	-1.832204	3.321498	0.004192	0.279789
-18.838863	-1.856754	3.331494	0.004131	0.279970
-18.442380	-1.887026	3.341491	0.004057	0.280185
-18.319857	-1.849344	3.351488	0.004034	0.280494
-18.192943	-1.841283	3.361485	0.004011	0.280655
-18.476306	-1.751210	3.371482	0.004064	0.280853
-17.804900	-1.828223	3.381478	0.003939	0.281085
-17.652495	-1.801253	3.391475	0.003910	0.281366
-17.413714	-1.798695	3.401472	0.003866	0.281602
-16.877052	-1.861708	3.411469	0.003766	0.281779
-16.740053	-1.841842	3.421466	0.003741	0.282008
-16.365477	-1.855996	3.431462	0.003671	0.282285
-16.305058	-1.824154	3.441459	0.003660	0.282504
-15.383439	-1.964978	3.451456	0.003489	0.282640
-15.136472	-1.946061	3.461453	0.003443	0.282967
-15.141896	-1.913975	3.471450	0.003444	0.283125
-14.895506	-1.927167	3.481446	0.003398	0.283286
-14.603009	-1.920825	3.491443	0.003344	0.283590
-14.055915	-1.985159	3.501440	0.003242	0.283769
-13.916245	-1.982606	3.511437	0.003216	0.283911
-13.841118	-1.933538	3.521434	0.003202	0.284230
-13.433280	-1.975804	3.531430	0.003126	0.284392
-13.797370	-1.871376	3.541427	0.003194	0.284586
-13.691468	-1.834898	3.551424	0.003174	0.284869
-12.978208	-1.913941	3.561421	0.003042	0.285126
-12.978935	-1.878512	3.571418	0.003042	0.285304
-12.649246	-1.891398	3.581414	0.002981	0.285542
-12.149881	-1.938810	3.591411	0.002888	0.285762
-11.577332	-2.005376	3.601408	0.002781	0.285951
-11.432877	-2.002264	3.611405	0.002754	0.286100
-11.419428	-1.946374	3.621402	0.002752	0.286394
-11.120576	-1.958973	3.631398	0.002696	0.286605
-11.209170	-1.903019	3.641395	0.002713	0.286805
-10.255415	-2.036911	3.651392	0.002536	0.287004
-9.964811	-2.044228	3.661389	0.002482	0.287233
-10.454928	-1.917429	3.671386	0.002573	0.287423
-9.663050	-2.016625	3.681382	0.002426	0.287647
-9.650320	-1.966307	3.691379	0.002423	0.287912
-9.426298	-1.971281	3.701376	0.002382	0.288091
-9.579147	-1.903085	3.711373	0.002410	0.288293
-9.326753	-1.887095	3.721370	0.002363	0.288603
-8.900867	-1.923174	3.731366	0.002284	0.288810
-8.414877	-1.976984	3.741363	0.002194	0.288983
-8.220141	-1.956427	3.751360	0.002157	0.289263
-8.341524	-1.886412	3.761357	0.002180	0.289502
-8.016019	-1.905985	3.771354	0.002120	0.289699
-7.746976	-1.911099	3.781350	0.002070	0.289918
-7.635438	-1.872583	3.791347	0.002049	0.290211
-6.604702	-2.010466	3.801344	0.001857	0.290457
-5.880326	-2.124258	3.811341	0.001722	0.290545
-6.119556	-2.035531	3.821338	0.001767	0.290770
-5.651334	-2.083090	3.831334	0.001680	0.290957
-6.032138	-1.978183	3.841331	0.001751	0.291134
-5.897942	-1.946279	3.851328	0.001726	0.291413
-5.372513	-1.995317	3.861325	0.001628	0.291643
-5.468236	-1.940911	3.871322	0.001646	0.291826
-5.562273	-1.879092	3.881318	0.001664	0.292048
-5.567290	-1.811459	3.891315	0.001665	0.292378
-5.181794	-1.834585	3.901312	0.001593	0.292610
-5.079411	-1.803385	3.911309	0.001574	0.292855
-4.972194	-1.771660	3.921306	0.001554	0.293108
-4.863462	-1.740831	3.931302	0.001534	0.293357
-4.706174	-1.713132	3.941299	0.001505	0.293634
-4.668543	-1.657210	3.951296	0.001498	0.293943
-4.126881	-1.700054	3.961293	0.001397	0.294216
-3.713930	-1.727875	3.971290	0.001320	0.294448
-3.531378	-1.711094	3.981286	0.001286	0.294693
-3.549989	-1.648389	3.991283	0.001290	0.294984
-3.527111	-1.595025	4.001280	0.001286	0.295266
-2.546529	-1.722874	4.011277	0.001103	0.295512
-2.889308	-1.607338	4.021274	0.001167	0.295772
-2.865631	-1.551550	4.031270	0.001163	0.296065
-2.991676	-1.467109	4.041267	0.001186	0.296366
-3.082184	-1.384956	4.051264	0.001203	0.296686
-2.458955	-1.438883	4.061261	0.001087	0.296975
-2.563139	-1.355999	4.071258	0.001107	0.297286
-2.384866	-1.323557	4.081254	0.001073	0.297601
-2.483744	-1.231367	4.091251	0.001092	0.297961
-2.105430	-1.239040	4.101248	0.001021	0.298257
-1.771684	-1.232839	4.111245	0.000959	0.298581
-1.816481	-1.155936	4.121242	0.000968	0.298914
-1.577875	-1.121399	4.131238	0.000923	0.299290
-1.042919	-1.157514	4.141235	0.000824	0.299585
-1.086312	-1.078176	4.151232	0.000832	0.299929
-1.128410	-0.995878	4.161229	0.000840	0.300289
-2.002903	-0.756531	4.171226	0.001003	0.300676
-1.730956	-0.736229	4.181222	0.000952	0.301011
-1.538306	-0.687111	4.191219	0.000916	0.301415
-1.311926	-0.638992	4.201216	0.000874	0.301842
-1.188524	-0.583749	4.211213	0.000851	0.302214
-1.014806	-0.536119	4.221210	0.000819	0.302593
-0.961869	-0.445481	4.231206	0.000809	0.303071
-0.359370	-0.479644	4.241203	0.000697	0.303430
-0.715304	-0.332391	4.251200	0.000763	0.303823
-1.180445	-0.137978	4.261197	0.000850	0.304346
-1.033197	-0.078437	4.271194	0.000823	0.304755
-0.683009	-0.040676	4.281190	0.000757	0.305236
-0.438446	0.009093	4.291187	0.000712	0.305682
-0.270947	0.068642	4.301184	0.000681	0.306107
-0.194414	0.155475	4.311181	0.000667	0.306583
0.000000	0.208984	4.321178	0.000630	0.307001

0.178725	0.465516	4.326182	0.000597	0.308360
0.381695	0.986448	4.331187	0.000559	0.310966
0.289640	1.847823	4.336192	0.000576	0.314872
0.444218	2.949833	4.341197	0.000546	0.320023
0.930281	4.271604	4.346202	0.000455	0.326336
1.977164	5.790088	4.351206	0.000259	0.333825
2.757943	7.664568	4.356211	0.000112	0.342453
3.313860	9.893068	4.361216	0.000007	0.352157
4.551171	12.302695	4.366221	-0.000224	0.362817
5.124765	15.159904	4.371226	-0.000333	0.374440
6.416680	18.213377	4.376230	-0.000576	0.386934
7.385358	21.673169	4.381235	-0.000758	0.400295
8.275929	25.491581	4.386240	-0.000926	0.414429
9.813589	29.544757	4.391245	-0.001215	0.429282
11.317028	33.955024	4.396250	-0.001498	0.444781
12.236621	38.841597	4.401254	-0.001672	0.460921
13.928293	43.935762	4.406259	-0.001991	0.477567
15.817833	49.346306	4.411264	-0.002346	0.494680
17.567220	55.157082	4.416269	-0.002676	0.512280
18.848475	61.385035	4.421274	-0.002918	0.530202
20.334209	67.916129	4.426278	-0.003199	0.548433
22.671188	74.613032	4.431283	-0.003638	0.566891
24.671725	81.686886	4.436288	-0.004016	0.585546
27.057594	88.996616	4.441293	-0.004464	0.604354
30.000527	96.501867	4.446298	-0.005017	0.623277
32.583192	104.342917	4.451302	-0.005503	0.642251
34.455480	112.577408	4.456307	-0.005857	0.661261
36.347930	121.007777	4.461312	-0.006215	0.680162
37.428630	129.801410	4.466317	-0.006422	0.699001
39.226325	138.627427	4.471322	-0.006762	0.717668
41.716120	147.509636	4.476326	-0.007232	0.736212
44.649972	156.458848	4.481331	-0.007784	0.754578
46.771129	165.683927	4.486336	-0.008185	0.772751
47.928489	175.204652	4.491341	-0.008406	0.790732
48.809855	184.826520	4.496346	-0.008577	0.808406
50.136126	194.435799	4.501350	-0.008830	0.825817
51.329309	204.118520	4.506355	-0.009058	0.842953
52.505273	213.806716	4.511360	-0.009284	0.859750
53.402563	223.575839	4.516365	-0.009457	0.876277
54.426091	233.305535	4.521370	-0.009654	0.892469
55.252002	243.082734	4.526374	-0.009814	0.908393
56.620346	252.724493	4.531379	-0.010075	0.923978
58.009116	262.357291	4.536384	-0.010340	0.939295
59.016428	272.040078	4.541389	-0.010534	0.954341
60.471744	281.582243	4.546394	-0.010811	0.969059
61.702525	291.157127	4.551398	-0.011046	0.983546
62.812515	300.727431	4.556403	-0.011259	0.997785
63.413542	310.294437	4.561408	-0.011377	1.011692
65.115617	319.622553	4.566413	-0.011700	1.025342
66.537838	328.951818	4.571418	-0.011971	1.038746
67.150328	338.394718	4.576422	-0.012091	1.051942
68.417236	347.662866	4.581427	-0.012333	1.064891
69.043069	356.989705	4.586432	-0.012456	1.077613
70.058764	366.192252	4.591437	-0.012651	1.090111
70.859933	375.381323	4.596442	-0.012806	1.102401
71.594391	384.539438	4.601446	-0.012948	1.114500
72.780616	393.558253	4.606451	-0.013175	1.126389
73.944045	402.536942	4.611456	-0.013398	1.138097
74.643644	411.594675	4.616461	-0.013534	1.149685
75.423474	420.559464	4.621466	-0.013685	1.161059
76.426591	429.438312	4.626470	-0.013877	1.172262
77.612378	438.249251	4.631475	-0.014104	1.183315
78.804832	447.015203	4.636480	-0.014331	1.194211
79.527874	455.853416	4.641485	-0.014472	1.204999
80.706981	464.567074	4.646490	-0.014697	1.215635
82.411454	473.168637	4.651494	-0.015020	1.226152
83.572088	481.864380	4.656499	-0.015242	1.236580
84.112860	490.607572	4.661504	-0.015348	1.246854
85.006085	499.277932	4.666509	-0.015520	1.257028
85.691455	507.939906	4.671514	-0.015653	1.267071
86.189403	516.620362	4.676518	-0.015751	1.277019
87.036857	525.197449	4.681523	-0.015915	1.286840
87.697091	533.799237	4.686528	-0.016043	1.296579
88.507830	542.349815	4.691533	-0.016200	1.306217
89.441608	550.930885	4.696538	-0.016379	1.315840
91.442650	559.205774	4.701542	-0.016757	1.325253
93.168108	567.586927	4.706547	-0.017084	1.334665
94.476897	575.970877	4.711552	-0.017333	1.343938
95.692952	584.423579	4.716557	-0.017565	1.353204
96.853873	592.835132	4.721562	-0.017786	1.362352
97.698460	601.337312	4.726566	-0.017949	1.371479
98.725709	609.765912	4.731571	-0.018146	1.380501
99.211337	618.265111	4.736576	-0.018242	1.389442
100.384500	626.622189	4.741581	-0.018466	1.398298
100.715249	635.100711	4.746586	-0.018533	1.407079
101.150575	643.562636	4.751590	-0.018619	1.415806
101.707494	651.962791	4.756595	-0.018728	1.424437
102.578843	660.296315	4.761600	-0.018896	1.433001
103.071068	668.676906	4.766605	-0.018993	1.441498
103.948709	676.986608	4.771610	-0.019162	1.449938
103.905433	685.462888	4.776614	-0.019159	1.458343
104.587650	693.768167	4.781619	-0.019292	1.466649
104.786468	702.193484	4.786624	-0.019334	1.474948
105.829464	710.397153	4.791629	-0.019534	1.483120
106.247786	718.735895	4.796634	-0.019617	1.491278
106.657438	727.040451	4.801638	-0.019699	1.499357
107.112646	735.360791	4.806643	-0.019789	1.507415
107.437480	743.661882	4.811648	-0.019855	1.515392
108.303163	751.881574	4.816653	-0.020021	1.523333
108.302116	760.257545	4.821658	-0.020026	1.531247
108.800383	768.521089	4.826662	-0.020124	1.539090
109.427534	776.758342	4.831667	-0.020247	1.546889
109.716791	785.040548	4.836672	-0.020306	1.554639
110.436030	793.243759	4.841677	-0.020445	1.562342
110.397346	801.579349	4.846682	-0.020443	1.570016
110.783072	809.818502	4.851686	-0.020520	1.577627
111.351123	818.032336	4.856691	-0.020631	1.585205
111.498404	826.331512	4.861696	-0.020664	1.592763
112.079276	834.501287	4.866701	-0.020778	1.600232
112.209764	842.781912	4.871706	-0.020807	1.607699
113.773573	850.816206	4.876710	-0.021104	1.615118
114.843225	858.990373	4.881715	-0.021308	1.622557
115.340488	867.245182	4.886720	-0.021406	1.629951
116.091814	875.465001	4.891725	-0.021551	1.637316
116.811622	883.632754	4.896730	-0.021691	1.644599
117.184133	891.879088	4.901734	-0.021765	1.651869
117.559573	900.119027	4.906739	-0.021840	1.659102
118.648693	908.180006	4.911744	-0.022048	1.666246
119.748705	916.329046	4.916749	-0.022259	1.673438
120.542301	924.504158	4.921754	-0.022412	1.680579
121.004939	932.745374	4.926758	-0.022503	1.687701
122.076309	940.892634	4.931763	-0.022708	1.694794
122.245535	949.149708	4.936768	-0.022745	1.701831
123.074264	957.343199	4.941773	-0.022904	1.708872
123.514046	965.572474	4.946778	-0.022991	1.715863
123.709615	973.806835	4.951782	-0.023033	1.722797
124.522025	981.943584	4.956787	-0.023190	1.729703
124.685485	990.190067	4.961792	-0.023226	1.736587
125.098114	998.381660	4.966797	-0.023308	1.743431
125.845562	1006.507910	4.971802	-0.023452	1.750238
125.879804	1014.764093	4.976806	-0.023464	1.757033
126.818122	1022.841334	4.981811	-0.023644	1.763771
127.020522	1031.055314	4.986816	-0.023687	1.770501
127.696867	1039.208335	4.991821	-0.023818	1.777216
128.008514	1047.399754	4.996826	-0.023881	1.783891
128.179245	1055.623597	5.001830	-0.023918	1.790549
128.993431	1063.724309	5.006835	-0.024075	1.797163
129.020575	1071.938885	5.011840	-0.024086	1.803747
130.189472	1079.957840	5.016845	-0.024308	1.810292
130.759844	1088.103625	5.021850	-0.024420	1.816840
131.351574	1096.236207	5.026854	-0.024535	1.823356
132.024229	1104.384192	5.031859	-0.024666	1.829871
132.729493	1112.485696	5.036864	-0.024802	1.836330
132.856947	1120.727615	5.041869	-0.024831	1.842807
133.493377	1128.850879	5.046874	-0.024955	1.849229
133.820050	1137.027124	5.051878	-0.025021	1.855633
134.713971	1145.105558	5.056883	-0.025193	1.862006
135.164626	1153.278268	5.061888	-0.025282	1.868378
135.634148	1161.431179	5.066893	-0.025375	1.874715
135.909647	1169.583774	5.071898	-0.025431	1.881008
136.279312	1177.714629	5.076902	-0.025505	1.887274
137.123606	1185.814003	5.081907	-0.025668	1.893550
137.887134	1193.897197	5.086912	-0.025815	1.899783
138.466120	1202.025411	5.091917	-0.025928	1.906009
139.041382	1210.166202	5.096922	-0.026041	1.912224
139.114592	1218.370733	5.101926	-0.026060	1.918408
139.607650	1226.490911	5.106931	-0.026157	1.924558
140.038574	1234.623514	5.111936	-0.026242	1.930689
140.882346	1242.703622	5.116941	-0.026405	1.936809
141.898938	1250.748833	5.121946	-0.026599	1.942902
142.156526	1258.943914	5.126950	-0.026652	1.949003
142.848613	1267.045319	5.131955	-0.026786	1.955063
143.502361	1275.108602	5.136960	-0.026913	1.961072
143.659888	1283.306001	5.141965	-0.026948	1.967107
143.862351	1291.494434	5.146970	-0.026991	1.973121
144.499627	1299.552286	5.151974	-0.027115	1.979069
144.972486	1307.664906	5.156979	-0.027208	1.985021
145.502942	1315.773862	5.161984	-0.027312	1.990959
146.101612	1323.881104	5.166989	-0.027429	1.996885
146.448110	1332.014302	5.171994	-0.027499	2.002785
146.714801	1340.164526	5.176998	-0.027554	2.008671
147.309794	1348.259150	5.182003	-0.027670	2.014535
147.825545	1356.351782	5.187008	-0.027771	2.020372
148.007221	1364.524787	5.192013	-0.027810	2.026214
148.628334	1372.615817	5.197018	-0.027931	2.032028
148.863229	1380.748560	5.202022	-0.027980	2.037813
149.528914	1388.791921	5.207027	-0.028109	2.043564
149.745433	1396.935353	5.212032	-0.028155	2.049322
150.037739	1405.053786	5.217037	-0.028214	2.055055
150.517994	1413.134264	5.222042	-0.028309	2.060764
151.348896	1421.156319	5.227046	-0.028469	2.066453
151.628103	1429.334775	5.232051	-0.028526	2.072178
152.068234	1437.407893	5.237056	-0.028613	2.077830
152.547316	1445.479166	5.242061	-0.028708	2.083470
153.181410	1453.574058	5.247066	-0.028831	2.089126
153.331599	1461.731109	5.252070	-0.028864	2.094761
154.236519	1469.769659	5.257075	-0.029038	2.100375
154.587083	1477.871364	5.262080	-0.029108	2.105962
155.570937	1485.936535	5.267085	-0.029297	2.111572
155.899818	1494.069388	5.272090	-0.029363	2.117148
156.591189	1502.102258	5.277094	-0.029497	2.122677
157.235434	1510.219686	5.282099	-0.029622	2.128244
157.476949	1518.343319	5.287104	-0.029673	2.133762
158.100647	1526.414525	5.292109	-0.029794	2.139266
158.414762	1534.518381	5.297114	-0.029858	2.144749
158.810451	1542.631730	5.302118	-0.029937	2.150232
159.192876	1550.739990	5.307123	-0.030013	2.155696
159.591238	1558.823300	5.312128	-0.030092	2.161131
160.274316	1566.890250	5.317133	-0.030225	2.166568
160.775713	1574.993162	5.322138	-0.030323	2.171998
160.768774	1583.140059	5.327142	-0.030327	2.177396
161.123365	1591.244027	5.332147	-0.030399	2.182786
161.657054	1599.290171	5.337152	-0.030503	2.188141
162.489398	1607.326549	5.342157	-0.030663	2.193505
162.723295	1615.448947	5.347162	-0.030712	2.198856
163.252404	1623.500968	5.352166	-0.030816	2.204175
164.059001	1631.535930	5.357171	-0.030971	2.209496
164.470711	1639.645531	5.362176	-0.031053	2.214816
164.856096	1647.761350	5.367181	-0.031130	2.220125
165.122750	1655.873377	5.372186	-0.031185	2.225407
165.530909	1663.961030	5.377190	-0.031266	2.230675
165.876707	1672.073492	5.382195	-0.031336	2.235940
166.127314	1680.155824	5.387200	-0.031388	2.241165
166.007781	1688.315705	5.392205	-0.031371	2.246393
166.364517	1696.379508	5.397210	-0.031443	2.251591
166.641600	1704.453552	5.402214	-0.031499	2.256777
167.499835	1712.443140	5.407219	-0.031664	2.261948
167.986320	1720.480403	5.412224	-0.031760	2.267105
169.083972	1728.510034	5.417229	-0.031970	2.272299
169.719938	1736.586533	5.422234	-0.032093	2.277469
170.122057	1744.655470	5.427238	-0.032173	2.282603
170.735408	1752.752243	5.432243	-0.032293	2.287761
171.264952	1760.829902	5.437248	-0.032397	2.292888
172.119086	1768.857229	5.442253	-0.032561	2.298000
172.663635	1776.936817	5.447258	-0.032668	2.303106
173.155930	1785.024429	5.452262	-0.032764	2.308202
173.896423	1793.087065	5.457267	-0.032907	2.313292
174.594775	1801.108714	5.462272	-0.033043	2.318341
175.243391	1809.178595	5.467277	-0.033169	2.323405
175.673881	1817.315632	5.472282	-0.033254	2.328481
175.874214	1825.431443	5.477286	-0.033297	2.333513
176.435827	1833.508429	5.482291	-0.033406	2.338540
176.804710	1841.567540	5.487296	-0.033480	2.343530
177.090686	1849.697899	5.492301	-0.033539	2.348545
177.662384	1857.745479	5.497306	-0.033650	2.353524
178.157369	1865.797923	5.502310	-0.033748	2.358488
178.604341	1873.877783	5.507315	-0.033836	2.363454
178.334075	1882.052923	5.512320	-0.033791	2.368408
178.959918	1890.068674	5.517325	-0.033913	2.373329
179.505447	1898.104103	5.522330	-0.034020	2.378245
180.163080	1906.109119	5.527334	-0.034147	2.383142
180.977197	1914.162507	5.532339	-0.034304	2.388070
181.481682	1922.243891	5.537344	-0.034403	2.392980
181.544148	1930.392779	5.542349	-0.034420	2.397884
181.677314	1938.473391	5.547354	-0.034450	2.402743
181.963656	1946.544459	5.552358	-0.034509	2.407599
182.716444	1954.578513	5.557363	-0.034654	2.412460
182.991990	1962.642726	5.562368	-0.034711	2.417291
183.156437	1970.756986	5.567373	-0.034747	2.422134
184.013583	1978.743520	5.572378	-0.034911	2.426945
184.514833	1986.809626	5.577382	-0.035010	2.431766
184.543442	1994.976236	5.582387	-0.035020	2.436600
185.042370	2002.972613	5.587392	-0.035118	2.441360
185.640758	2010.984226	5.592397	-0.035235	2.446128
186.057312	2019.064602	5.597402	-0.035318	2.450913
186.439939	2027.133852	5.602406	-0.035394	2.455679
186.851170	2035.223002	5.607411	-0.035476	2.460449
186.603753	2043.359767	5.612416	-0.035435	2.465188
187.216809	2051.383693	5.617421	-0.035555	2.469917
187.806106	2059.402914	5.622426	-0.035670	2.474633
188.261004	2067.415114	5.627430	-0.035759	2.479325
188.492339	2075.498434	5.632435	-0.035808	2.484033
188.875641	2083.569571	5.637440	-0.035884	2.488736
189.157557	2091.669996	5.642445	-0.035942	2.493440
189.247543	2099.770822	5.647450	-0.035964	2.498120
189.975021	2107.734543	5.652454	-0.036105	2.502760
190.144962	2115.876977	5.657459	-0.036142	2.507453
190.437436	2123.925208	5.662464	-0.036201	2.512092
190.813138	2131.981829	5.667469	-0.036276	2.516733
191.034538	2140.051920	5.672474	-0.036323	2.521362
191.282003	2148.084880	5.677478	-0.036374	2.525964
191.399978	2156.201741	5.682483	-0.036401	2.530595
192.006859	2164.171145	5.687488	-0.036519	2.535169
192.602623	2172.187874	5.692493	-0.036636	2.539761
192.756742	2180.273668	5.697498	-0.036669	2.544352
192.785354	2188.394393	5.702502	-0.036680	2.548945
193.519935	2196.379703	5.707507	-0.036822	2.553505
193.748016	2204.468281	5.712512	-0.036870	2.558077
193.766263	2212.556282	5.717517	-0.036878	2.562627
194.214066	2220.597032	5.722522	-0.036967	2.567172
194.113777	2228.734256	5.727526	-0.036953	2.571724
195.256144	2236.638469	5.732531	-0.037171	2.576226
195.665434	2244.690967	5.737536	-0.037253	2.580751
195.850324	2252.791575	5.742541	-0.037292	2.585279
196.315042	2260.861331	5.747546	-0.037384	2.589801
196.692944	2268.996665	5.752550	-0.037460	2.594346
197.497250	2276.956416	5.757555	-0.037615	2.598815
197.507469	2285.021458	5.762560	-0.037622	2.603279
197.739940	2293.079528	5.767565	-0.037670	2.607748
198.479059	2301.089481	5.772570	-0.037813	2.612217
198.863218	2309.128804	5.777574	-0.037890	2.616669
199.055628	2317.225350	5.782579	-0.037931	2.621133
199.435518	2325.249510	5.787584	-0.038007	2.625562
199.586015	2333.348544	5.792589	-0.038040	2.630009
199.562418	2341.457037	5.797594	-0.038041	2.634441
199.875513	2349.451812	5.802598	-0.038104	2.638827
200.610767	2357.446731	5.807603	-0.038246	2.643235
200.813766	2365.519600	5.812608	-0.038289	2.647641
200.949023	2373.593999	5.817613	-0.038320	2.652036
201.436632	2381.643017	5.822618	-0.038416	2.656434
201.514382	2389.703067	5.827622	-0.038436	2.660803
202.030681	2397.728839	5.832627	-0.038537	2.665175
201.940090	2405.849579	5.837632	-0.038525	2.669551
202.871544	2413.799718	5.842637	-0.038704	2.673896
203.318141	2421.840704	5.847642	-0.038792	2.678250
203.210291	2429.930220	5.852646	-0.038777	2.682587
203.296979	2438.030018	5.857651	-0.038799	2.686935
203.088014	2446.165001	5.862656	-0.038765	2.691275
203.498277	2454.171620	5.867661	-0.038847	2.695580
204.206457	2462.121145	5.872666	-0.038984	2.699868
204.721420	2470.090727	5.877670	-0.039085	2.704146
204.986411	2478.183983	5.882675	-0.039139	2.708467
204.965399	2486.298408	5.887680	-0.039141	2.712774
205.397447	2494.308591	5.892685	-0.039226	2.717048
205.979900	2502.318253	5.897690	-0.039340	2.721325
205.922132	2510.398929	5.902694	-0.039334	2.725591
206.208919	2518.485222	5.907699	-0.039393	2.729876
206.647560	2526.505102	5.912704	-0.039480	2.734128
206.892027	2534.575222	5.917709	-0.039530	2.738388
207.447881	2542.564930	5.922714	-0.039639	2.742619
207.784417	2550.610147	5.927718	-0.039707	2.746858
207.841903	2558.767471	5.932723	-0.039723	2.751132
208.554310	2566.770600	5.937728	-0.039861	2.755360
208.664197	2574.814244	5.942733	-0.039886	2.759565
208.704218	2582.897692	5.947738	-0.039899	2.763779
208.773759	2590.941379	5.952742	-0.039917	2.767969
209.446746	2598.942270	5.957747	-0.040048	2.772167
209.510656	2607.011833	5.962752	-0.040065	2.776356
209.872739	2615.022339	5.967757	-0.040137	2.780527
210.693480	2622.983333	5.972762	-0.040295	2.784694
210.686531	2631.095577	5.977766	-0.040299	2.788883
210.900191	2639.161460	5.982771	-0.040344	2.793054
211.309598	2647.191761	5.987776	-0.040426	2.797213
211.551150	2655.233789	5.992781	-0.040476	2.801362
211.772345	2663.279907	5.997786	-0.040522	2.805505
211.943701	2671.340193	6.002790	-0.040559	2.809646
212.345774	2679.392394	6.007795	-0.040640	2.813791
213.159901	2687.341672	6.012800	-0.040796	2.817901
213.352016	2695.414207	6.017805	-0.040837	2.822032
213.775460	2703.468274	6.022810	-0.040921	2.826160
213.772306	2711.574365	6.027814	-0.040926	2.830284
214.047883	2719.610985	6.032819	-0.040982	2.834383
214.203681	2727.639913	6.037824	-0.041017	2.838465
214.742685	2735.645763	6.042829	-0.041122	2.842552
215.061522	2743.695462	6.047834	-0.041187	2.846642
214.964530	2751.781600	6.052838	-0.041174	2.850721
215.432659	2759.804832	6.057843	-0.041266	2.854794
215.508351	2767.876462	6.062848	-0.041286	2.858864
215.949314	2775.854090	6.067853	-0.041373	2.862901
216.480333	2783.884634	6.072858	-0.041477	2.866964
216.579081	2791.993337	6.077862	-0.041501	2.871036
216.914861	2800.044982	6.082867	-0.041568	2.875088
217.074577	2808.077467	6.087872	-0.041603	2.879113
217.384980	2816.081768	6.092877	-0.041666	2.883128
218.369882	2824.027077	6.097882	-0.041855	2.887145
218.144416	2832.172151	6.102886	-0.041818	2.891189
218.674292	2840.203529	6.107891	-0.041922	2.895212
218.684122	2848.290170	6.112896	-0.041929	2.899228
219.469043	2856.204328	6.117901	-0.042080	2.903196
219.378345	2864.363146	6.122906	-0.042069	2.907231
219.794034	2872.387743	6.127910	-0.042151	2.911223
220.350028	2880.434548	6.132915	-0.042260	2.915227
220.588932	2888.443685	6.137920	-0.042309	2.919190
221.228434	2896.434021	6.142925	-0.042434	2.923159
221.750497	2904.478426	6.147930	-0.042536	2.927144
221.701329	2912.568562	6.152934	-0.042532	2.931115
222.096936	2920.585567	6.157939	-0.042611	2.935068
222.608607	2928.593810	6.162944	-0.042711	2.939018
223.058166	2936.593110	6.167949	-0.042800	2.942955
223.696680	2944.615262	6.172954	-0.042924	2.946908
223.595534	2952.791644	6.177958	-0.042911	2.950891
223.895089	2960.830059	6.182963	-0.042972	2.954823
224.496529	2968.796969	6.187968	-0.043089	2.958730
225.153147	2976.751369	6.192973	-0.043216	2.962630
225.962987	2984.754037	6.197978	-0.043372	2.966555
226.096079	2992.852139	6.202982	-0.043402	2.970486
226.272856	3000.938885	6.207987	-0.043441	2.974409
226.901796	3008.934513	6.212992	-0.043563	2.978306
226.890134	3017.057342	6.217997	-0.043566	2.982225
227.171763	3025.112598	6.223002	-0.043624	2.986122
227.285837	3033.172538	6.228006	-0.043650	2.990008
227.812343	3041.197464	6.233011	-0.043753	2.993893
227.911798	3049.257380	6.238016	-0.043777	2.997768
228.311553	3057.231167	6.243021	-0.043857	3.001612
228.720307	3065.260751	6.248026	-0.043938	3.005478
229.083196	3073.258099	6.253030	-0.044011	3.009321
229.777578	3081.276397	6.258035	-0.044145	3.013186
230.348791	3089.305342	6.263040	-0.044257	3.017045
230.615708	3097.379742	6.268045	-0.044311	3.020905
230.597538	3105.475729	6.273050	-0.044313	3.024756
230.613958	3113.531700	6.278054	-0.044322	3.028585
231.439435	3121.498147	6.283059	-0.044480	3.032406
231.335184	3129.607144	6.288064	-0.044466	3.036245
232.066889	3137.538282	6.293069	-0.044608	3.040035
232.154885	3145.623811	6.298074	-0.044629	3.043862
232.141582	3153.699069	6.303078	-0.044632	3.047675
232.485956	3161.761671	6.308083	-0.044701	3.051494
233.005481	3169.745340	6.313088	-0.044803	3.055280
233.432838	3177.759399	6.318093	-0.044888	3.059070
233.836640	3185.796713	6.323098	-0.044968	3.062866
233.728331	3193.889953	6.328102	-0.044953	3.066658
234.479601	3201.904932	6.333107	-0.045098	3.070451
234.825782	3209.968029	6.338112	-0.045168	3.074242
234.960094	3217.986912	6.343117	-0.045198	3.077997
235.964135	3225.924223	6.348122	-0.045390	3.081751
235.700167	3234.029345	6.353126	-0.045347	3.085518
236.119174	3242.056170	6.358131	-0.045430	3.089277
236.633414	3250.067811	6.363136	-0.045531	3.093028
236.556156	3258.159225	6.368141	-0.045521	3.096784
237.055198	3266.164035	6.373146	-0.045620	3.100522
237.569692	3274.117887	6.378150	-0.045721	3.104233
237.562207	3282.252577	6.383155	-0.045724	3.107998
237.457622	3290.367107	6.388160	-0.045710	3.111745
237.729133	3298.371512	6.393165	-0.045766	3.115455
238.425761	3306.331881	6.398170	-0.045901	3.119159
238.667598	3314.326166	6.403174	-0.045951	3.122853
238.741136	3322.418239	6.408179	-0.045970	3.126580
239.055756	3330.478843	6.413184	-0.046034	3.130299
239.893284	3338.422689	6.418189	-0.046195	3.133985
240.163260	3346.514090	6.423194	-0.046250	3.137707
240.613645	3354.498351	6.428198	-0.046339	3.141384
241.273610	3362.499348	6.433203	-0.046467	3.145074
241.203442	3370.638658	6.438208	-0.046460	3.148789
241.219059	3378.684584	6.443213	-0.046468	3.152462
241.389333	3386.773269	6.448218	-0.046505	3.156156
241.960813	3394.696061	6.453222	-0.046616	3.159789
242.174781	3402.718444	6.458227	-0.046661	3.163447
242.777916	3410.714023	6.463232	-0.046779	3.167106
242.672449	3418.833453	6.468237	-0.046764	3.170785
243.384740	3426.809795	6.473242	-0.046902	3.174431
243.457027	3434.877554	6.478246	-0.046921	3.178086
243.991724	3442.882589	6.483251	-0.047025	3.181728
244.201588	3450.925240	6.488256	-0.047070	3.185370
244.202558	3459.009274	6.493261	-0.047075	3.189016
244.771147	3467.009398	6.498266	-0.047186	3.192645
244.615956	3475.106308	6.503270	-0.047162	3.196283
245.179106	3483.073508	6.508275	-0.047272	3.199889
245.633510	3491.047245	6.513280	-0.047362	3.203488
245.195213	3499.221215	6.518285	-0.047286	3.207136
246.499514	3507.083612	6.523290	-0.047534	3.210714
246.643862	3515.139146	6.528294	-0.047566	3.214325
246.970181	3523.203195	6.533299	-0.047632	3.217943
247.096047	3531.247338	6.538304	-0.047660	3.221540
247.300358	3539.267156	6.543309	-0.047704	3.225126
247.913129	3547.301376	6.548314	-0.047823	3.228731
248.189460	3555.328348	6.553318	-0.047880	3.232314
248.796606	3563.337991	6.558323	-0.047998	3.235900
249.488452	3571.279878	6.563328	-0.048132	3.239455
249.220163	3579.414280	6.568333	-0.048087	3.243051
249.810813	3587.406307	6.573338	-0.048202	3.246616
250.073760	3595.447343	6.578342	-0.048256	3.250185
249.967073	3603.555995	6.583347	-0.048242	3.253765
250.139970	3611.621228	6.588352	-0.048279	3.257333
250.297229	3619.640903	6.593357	-0.048314	3.260876
250.931883	3627.583131	6.598362	-0.048437	3.264401
251.361808	3635.627091	6.603366	-0.048522	3.267959
251.485788	3643.701279	6.608371	-0.048551	3.271513
251.760686	3651.703492	6.613376	-0.048607	3.275038
251.807754	3659.768249	6.618381	-0.048621	3.278578
251.996813	3667.834380	6.623386	-0.048661	3.282120
252.506183	3675.769988	6.628390	-0.048761	3.285613
252.684542	3683.816805	6.633395	-0.048800	3.289139
253.322881	3691.843855	6.638400	-0.048924	3.292670
253.038449	3699.949764	6.643405	-0.048876	3.296195
253.593058	3707.879555	6.648410	-0.048984	3.299673
254.183991	3715.902940	6.653414	-0.049100	3.303189
254.524923	3723.953538	6.658419	-0.049168	3.306704
255.327602	3731.921466	6.663424	-0.049323	3.310197
254.988557	3740.061785	6.668429	-0.049265	3.313716
255.426155	3748.091611	6.673434	-0.049352	3.317214
255.368921	3756.150823	6.678438	-0.049346	3.320701
255.827198	3764.095687	6.683443	-0.049437	3.324156
256.640929	3772.072157	6.688448	-0.049593	3.327634
256.861288	3780.140053	6.693453	-0.049640	3.331125
257.448067	3788.197629	6.698458	-0.049754	3.334622
257.768766	3796.205675	6.703462	-0.049819	3.338084
257.598931	3804.317270	6.708467	-0.049793	3.341568
257.449117	3812.375168	6.713472	-0.049770	3.345025
258.539048	3820.256871	6.718477	-0.049978	3.348451
258.947106	3828.350747	6.723482	-0.050059	3.351938
259.211747	3836.349238	6.728486	-0.050114	3.355376
259.186966	3844.447871	6.733491	-0.050114	3.358842
259.518782	3852.468119	6.738496	-0.050181	3.362284
259.499470	3860.523777	6.743501	-0.050183	3.365724
259.789531	3868.535083	6.748506	-0.050242	3.369154
259.601566	3876.639512	6.753510	-0.050212	3.372601
260.651913	3884.550790	6.758515	-0.050413	3.376009
260.747791	3892.614900	6.763520	-0.050436	3.379444
260.821940	3900.629610	6.768525	-0.050455	3.382853
261.348579	3908.653903	6.773530	-0.050558	3.386279
261.073170	3916.741574	6.778534	-0.050512	3.389699
261.801962	3924.726784	6.783539	-0.050653	3.393109
261.940541	3932.806337	6.788544	-0.050684	3.396533
262.768436	3940.695618	6.793549	-0.050843	3.399899
263.024339	3948.750565	6.798554	-0.050896	3.403311
263.409945	3956.754582	6.803558	-0.050973	3.406702
263.588067	3964.846607	6.808563	-0.051012	3.410120
264.163714	3972.813808	6.813568	-0.051124	3.413496
264.433555	3980.838757	6.818573	-0.051179	3.416882
264.510595	3988.963106	6.823578	-0.051199	3.420299
264.438017	3996.967599	6.828582	-0.051191	3.423657
264.487372	4005.044909	6.833587	-0.051205	3.427047
265.362773	4013.014175	6.838592	-0.051373	3.430418
265.610566	4021.028416	6.843597	-0.051424	3.433781
265.739794	4029.100097	6.848602	-0.051454	3.437161
266.033526	4037.088374	6.853606	-0.051514	3.440509
266.588998	4045.056146	6.858611	-0.051622	3.443854
266.834897	4053.139931	6.863616	-0.051673	3.447233
267.445112	4061.080997	6.868621	-0.051792	3.450562
267.374278	4069.230929	6.873626	-0.051784	3.453951
267.162251	4077.323800	6.878630	-0.051750	3.457309
267.629700	4085.298103	6.883635	-0.051842	3.460637
267.674718	4093.289985	6.888640	-0.051855	3.463955
267.790737	4101.362882	6.893645	-0.051882	3.467305
268.226441	4109.387485	6.898650	-0.051969	3.470643
268.124489	4117.423632	6.903654	-0.051955	3.473965
268.723884	4125.387241	6.908659	-0.052072	3.477277
268.513344	4133.489170	6.913664	-0.052038	3.480615
268.840556	4141.425253	6.918669	-0.052104	3.483900
269.624508	4149.436867	6.923674	-0.052255	3.487228
269.787520	4157.474417	6.928678	-0.052290	3.490543
270.364024	4165.466130	6.933683	-0.052403	3.493850
270.150577	4173.605456	6.938688	-0.052368	3.497188
270.492781	4181.562195	6.943693	-0.052437	3.500466
270.790075	4189.580378	6.948698	-0.052498	3.503765
271.088988	4197.607658	6.953702	-0.052559	3.507064
271.555414	4205.627125	6.958707	-0.052651	3.510362
272.024020	4213.645024	6.963712	-0.052743	3.513657
272.445824	4221.659064	6.968717	-0.052827	3.516945
272.958527	4229.653025	6.973722	-0.052927	3.520225
273.556540	4237.659502	6.978726	-0.053044	3.523510
273.452046	4245.740793	6.983731	-0.053030	3.526800
273.551475	4253.868196	6.988736	-0.053053	3.530112
273.671488	4261.900317	6.993741	-0.053081	3.533382
273.788229	4269.969405	6.998746	-0.053108	3.536665
274.429075	4277.841700	7.003750	-0.053232	3.539881
275.133254	4285.822851	7.008755	-0.053369	3.543140
275.197527	4293.957196	7.013760	-0.053386	3.546438
275.465717	4301.922271	7.018765	-0.053441	3.549671
275.989319	4310.013449	7.023770	-0.053544	3.552959
276.040564	4318.082682	7.028774	-0.053558	3.556221
276.242557	4326.008628	7.033779	-0.053601	3.559427
276.339519	4334.047357	7.038784	-0.053624	3.562673
276.473529	4342.085239	7.043789	-0.053655	3.565916
276.931442	4350.074258	7.048794	-0.053745	3.569146
276.360448	4358.218832	7.053798	-0.053644	3.572405
276.850453	4366.186017	7.058803	-0.053740	3.575622
277.231513	4374.216217	7.063808	-0.053816	3.578857
277.661913	4382.191784	7.068813	-0.053902	3.582069
277.477785	4390.292963	7.073818	-0.053873	3.585311
277.724233	4398.279705	7.078822	-0.053924	3.588516
277.954953	4406.299075	7.083827	-0.053972	3.591731
278.477585	4414.293231	7.088832	-0.054074	3.594942
278.474964	4422.340530	7.093837	-0.054079	3.598155
278.992728	4430.348166	7.098842	-0.054181	3.601365
279.502256	4438.276035	7.103846	-0.054281	3.604540
279.672006	4446.387337	7.108851	-0.054318	3.607776
279.870384	4454.455249	7.113856	-0.054360	3.610992
280.092344	4462.462740	7.118861	-0.054406	3.614181
280.483438	4470.500532	7.123866	-0.054484	3.617385
280.597736	4478.511349	7.128870	-0.054511	3.620567
280.624017	4486.549801	7.133875	-0.054521	3.623755
281.378609	4494.528761	7.138880	-0.054666	3.626938
281.807007	4502.559790	7.143885	-0.054751	3.630128
281.885225	4510.624721	7.148890	-0.054771	3.633320
281.842033	4518.691218	7.153894	-0.054768	3.636505
282.588588	4526.578811	7.158899	-0.054912	3.639640
282.371221	4534.715389	7.163904	-0.054877	3.642843
282.739449	4542.699488	7.168909	-0.054951	3.645999
283.262757	4550.672595	7.173914	-0.055054	3.649153
283.738493	4558.711771	7.178918	-0.055147	3.652328
283.627002	4566.800970	7.183923	-0.055132	3.655504
283.809004	4574.809803	7.188928	-0.055171	3.658654
284.253023	4582.786641	7.193933	-0.055259	3.661795
284.154374	4590.859300	7.198938	-0.055245	3.664957
284.415591	4598.878029	7.203942	-0.055299	3.668105
284.319294	4606.989973	7.208947	-0.055287	3.671276
284.730994	4614.949214	7.213952	-0.055368	3.674399
284.669553	4622.975162	7.218957	-0.055362	3.677533
285.436350	4630.932693	7.223962	-0.055510	3.680659
285.731266	4638.912010	7.228966	-0.055570	3.683779
286.048942	4646.997680	7.233971	-0.055635	3.686938
286.047247	4655.072048	7.238976	-0.055639	3.690081
286.266957	4663.063608	7.243981	-0.055686	3.693195
286.590127	4671.128958	7.248986	-0.055751	3.696338
286.882447	4679.101251	7.253990	-0.055810	3.699441
286.937203	4687.155121	7.258995	-0.055826	3.702567
287.421521	4695.167685	7.264000	-0.055921	3.705686
287.742690	4703.131198	7.269005	-0.055986	3.708778
288.286696	4711.231123	7.274010	-0.056093	3.711927
288.587670	4719.253357	7.279014	-0.056154	3.715036
288.341087	4727.309043	7.284019	-0.056113	3.718142
288.768557	4735.305781	7.289024	-0.056198	3.721240
289.483299	4743.165737	7.294029	-0.056336	3.724289
289.941387	4751.239787	7.299034	-0.056427	3.727412
290.302937	4759.267926	7.304038	-0.056499	3.730513
289.997365	4767.380573	7.309043	-0.056448	3.733626
290.826105	4775.357759	7.314048	-0.056607	3.736713
290.669315	4783.402634	7.319053	-0.056583	3.739799
290.957017	4791.429395	7.324058	-0.056642	3.742886
290.778476	4799.506033	7.329062	-0.056614	3.745978
290.978110	4807.499727	7.334067	-0.056656	3.749046
291.011156	4815.573572	7.339072	-0.056667	3.752137
290.984945	4823.549279	7.344077	-0.056668	3.755187
291.491399	4831.547365	7.349082	-0.056767	3.758256
292.099166	4839.499159	7.354086	-0.056885	3.761307
292.358603	4847.450282	7.359091	-0.056939	3.764347
293.165746	4855.520014	7.364096	-0.057094	3.767443
293.015401	4863.602093	7.369101	-0.057072	3.770518
293.278873	4871.680331	7.374106	-0.057126	3.773598
293.759245	4879.652344	7.379110	-0.057221	3.776641
294.099831	4887.637258	7.384115	-0.057289	3.779683
294.507393	4895.670666	7.389120	-0.057370	3.782743
294.492331	4903.732019	7.394125	-0.057373	3.785801
295.133315	4911.766773	7.399130	-0.057497	3.788861
295.121864	4919.829527	7.404134	-0.057500	3.791915
295.475819	4927.811973	7.409139	-0.057571	3.794944
295.876663	4935.811306	7.414144	-0.057651	3.797977
295.753188	4943.911201	7.419149	-0.057633	3.801035
295.682160	4951.906830	7.424154	-0.057625	3.804052
295.634196	4959.952094	7.429158	-0.057622	3.807085
296.491542	4967.885259	7.434163	-0.057786	3.810095
296.577970	4975.932044	7.439168	-0.057808	3.813127
296.848601	4983.941024	7.444173	-0.057863	3.816147
297.164952	4991.978657	7.449178	-0.057927	3.819176
297.460113	4999.992491	7.454182	-0.057987	3.822194
297.424976	5008.018284	7.459187	-0.057986	3.825206
297.864158	5016.112217	7.464192	-0.058073	3.828252
297.851450	5024.144484	7.469197	-0.058076	3.831262
298.316179	5032.087420	7.474202	-0.058168	3.834247
299.242726	5040.047222	7.479206	-0.058345	3.837246
299.522632	5048.070679	7.484211	-0.058403	3.840252
299.824856	5056.125166	7.489216	-0.058464	3.843268
300.330116	5064.127478	7.494221	-0.058563	3.846266
299.986755	5072.250682	7.499226	-0.058505	3.849289
300.145052	5080.288349	7.504230	-0.058539	3.852288
300.615366	5088.252365	7.509235	-0.058632	3.855265
301.077251	5096.266870	7.514240	-0.058723	3.858257
301.147775	5104.314348	7.519245	-0.058741	3.861251
301.596662	5112.247397	7.524250	-0.058830	3.864208
302.048230	5120.327894	7.529254	-0.058919	3.867218
302.078599	5128.395755	7.534259	-0.058930	3.870212
302.339528	5136.526830	7.539264	-0.058984	3.873231
302.195676	5144.542901	7.544269	-0.058963	3.876197
302.933178	5152.427170	7.549274	-0.059105	3.879131
303.114858	5160.438218	7.554278	-0.059144	3.882097
303.462209	5168.391346	7.559283	-0.059214	3.885044
303.730656	5176.432846	7.564288	-0.059269	3.888019
303.852630	5184.488705	7.569293	-0.059297	3.890993
303.991082	5192.544801	7.574298	-0.059328	3.893967
304.121239	5200.553320	7.579302	-0.059357	3.896920
304.576893	5208.536646	7.584307	-0.059447	3.899868
304.278177	5216.621561	7.589312	-0.059397	3.902836
304.306510	5224.612377	7.594317	-0.059407	3.905774
305.413170	5232.542527	7.599322	-0.059619	3.908708
305.612827	5240.641924	7.604326	-0.059661	3.911685
305.889304	5248.604654	7.609331	-0.059718	3.914611
305.807703	5256.717011	7.614336	-0.059708	3.917582
306.141065	5264.729843	7.619341	-0.059775	3.920522
306.398254	5272.671790	7.624346	-0.059828	3.923433
306.640175	5280.754668	7.629350	-0.059878	3.926393
307.111754	5288.694045	7.634355	-0.059971	3.929303
307.695683	5296.779919	7.639360	-0.060085	3.932266
307.695974	5304.781049	7.644365	-0.060090	3.935185
308.088119	5312.810583	7.649370	-0.060168	3.938119
308.552285	5320.884565	7.654374	-0.060260	3.941069
308.768104	5328.827458	7.659379	-0.060305	3.943964
309.026896	5336.932939	7.664384	-0.060359	3.946917
309.159329	5344.919599	7.669389	-0.060389	3.949822
309.670308	5352.949643	7.674394	-0.060489	3.952747
309.668699	5360.969750	7.679398	-0.060494	3.955658
309.583275	5369.021547	7.684403	-0.060483	3.958576
309.966189	5377.068558	7.689408	-0.060560	3.961499
310.165461	5384.963574	7.694413	-0.060602	3.964361
310.444434	5393.066700	7.699418	-0.060659	3.967298
310.565452	5401.111271	7.704422	-0.060687	3.970208
310.837212	5409.067006	7.709427	-0.060743	3.973087
311.465652	5417.107880	7.714432	-0.060865	3.976002
311.660268	5425.090596	7.719437	-0.060906	3.978885
311.984252	5433.148219	7.724442	-0.060972	3.981795
312.035472	5441.119439	7.729446	-0.060986	3.984667
312.089941	5449.203003	7.734451	-0.061002	3.987578
312.492008	5457.227022	7.739456	-0.061082	3.990471
311.991819	5465.291933	7.744461	-0.060994	3.993361
312.358031	5473.312976	7.749466	-0.061067	3.996248
312.392788	5481.257532	7.754470	-0.061079	3.999100
313.029041	5489.259193	7.759475	-0.061203	4.001981
313.029393	5497.295373	7.764480	-0.061208	4.004861
313.240913	5505.268923	7.769485	-0.061252	4.007720
313.762177	5513.347115	7.774490	-0.061355	4.010620
313.686249	5521.372952	7.779494	-0.061346	4.013489
313.809588	5529.405680	7.784499	-0.061374	4.016361
314.161534	5537.423082	7.789504	-0.061444	4.019230
314.213365	5545.429646	7.794509	-0.061459	4.022088
314.553695	5553.427742	7.799514	-0.061528	4.024946
314.557219	5561.500618	7.804518	-0.061534	4.027822
315.107510	5569.451629	7.809523	-0.061641	4.030662
315.136009	5577.597280	7.814528	-0.061652	4.033561
315.012448	5585.661724	7.819533	-0.061634	4.036426
315.917059	5593.496417	7.824538	-0.061808	4.039225
316.099092	5601.578784	7.829542	-0.061847	4.042097
316.080649	5609.543045	7.834547	-0.061848	4.044923
316.517143	5617.551604	7.839552	-0.061935	4.047769
316.643264	5625.590349	7.844557	-0.061964	4.050619
317.096930	5633.602696	7.849562	-0.062053	4.053463
317.449931	5641.663256	7.854566	-0.062124	4.056320
317.496410	5649.589378	7.859571	-0.062138	4.059123
317.437343	5657.775778	7.864576	-0.062132	4.062014
317.859956	5665.678153	7.869581	-0.062216	4.064811
317.981530	5673.773558	7.874586	-0.062244	4.067669
318.547036	5681.741335	7.879590	-0.062354	4.070486
318.722070	5689.772382	7.884595	-0.062392	4.073318
319.016284	5697.854582	7.889600	-0.062452	4.076168
318.635262	5705.839845	7.894605	-0.062386	4.078971
318.957563	5713.854034	7.899610	-0.062452	4.081794
319.413271	5721.806963	7.904614	-0.062542	4.084595
319.977297	5729.823284	7.909619	-0.062652	4.087417
320.425898	5737.883139	7.914624	-0.062740	4.090251
320.896273	5745.837413	7.919629	-0.062833	4.093047
321.320470	5753.916016	7.924634	-0.062917	4.095883
320.946339	5761.983237	7.929638	-0.062853	4.098702
321.115517	5770.003301	7.934643	-0.062890	4.101510
321.184384	5778.015155	7.939648	-0.062908	4.104312
321.593886	5786.025879	7.944653	-0.062989	4.107117
321.543636	5794.058099	7.949658	-0.062985	4.109920
322.300449	5802.068797	7.954662	-0.063131	4.112726
322.501403	5810.044766	7.959667	-0.063174	4.115509
322.409437	5818.139148	7.964672	-0.063162	4.118328
322.467650	5826.155969	7.969677	-0.063178	4.121120
323.436036	5834.041041	7.974682	-0.063363	4.123877
323.448516	5842.107523	7.979686	-0.063371	4.126682
324.099847	5850.075538	7.984691	-0.063497	4.129459
324.487892	5858.206007	7.989696	-0.063575	4.132287
324.548524	5866.182916	7.994701	-0.063591	4.135056
324.756172	5874.229821	7.999706	-0.063635	4.137849
325.074791	5882.225747	8.004710	-0.063699	4.140624
325.406884	5890.144591	8.009715	-0.063766	4.143370
326.058472	5898.211104	8.014720	-0.063893	4.146170
325.670501	5906.288070	8.019725	-0.063826	4.148958
326.046201	5914.352629	8.024730	-0.063901	4.151749
326.165355	5922.353635	8.029734	-0.063928	4.154514
326.423101	5930.308749	8.034739	-0.063981	4.157263
326.474887	5938.402691	8.039744	-0.063996	4.160055
326.753248	5946.358790	8.044749	-0.064053	4.162800
327.034874	5954.370017	8.049754	-0.064111	4.165563
327.192377	5962.432011	8.054758	-0.064145	4.168339
327.666145	5970.427234	8.059763	-0.064239	4.171095
327.772695	5978.473804	8.064768	-0.064264	4.173862
327.622460	5986.562184	8.069773	-0.064241	4.176639
328.021010	5994.528191	8.074778	-0.064321	4.179378
327.841783	6002.553627	8.079782	-0.064292	4.182129
328.241872	6010.506597	8.084787	-0.064372	4.184860
328.576497	6018.600314	8.089792	-0.064440	4.187637
328.325216	6026.643209	8.094797	-0.064398	4.190387
328.726994	6034.682497	8.099802	-0.064478	4.193142
329.053657	6042.655829	8.104806	-0.064544	4.195872
329.578697	6050.575641	8.109811	-0.064647	4.198584
329.972448	6058.655243	8.114816	-0.064725	4.201347
330.173113	6066.556459	8.119821	-0.064768	4.204046
330.571343	6074.643979	8.124826	-0.064847	4.206808
330.878195	6082.648381	8.129830	-0.064909	4.209539
330.658880	6090.772721	8.134835	-0.064874	4.212303
331.136366	6098.761033	8.139840	-0.064968	4.215027
331.433271	6106.778062	8.144845	-0.065028	4.217757
331.458186	6114.817519	8.149850	-0.065038	4.220490
331.412334	6122.843341	8.154854	-0.065035	4.223215
331.526498	6130.825039	8.159859	-0.065061	4.225926
331.874775	6138.850480	8.164864	-0.065131	4.228652
331.974793	6146.877144	8.169869	-0.065155	4.231374
332.239524	6154.879868	8.174874	-0.065210	4.234088
332.828637	6162.869384	8.179878	-0.065324	4.236799
332.631116	6170.889665	8.184883	-0.065293	4.239511
332.989755	6178.948611	8.189888	-0.065365	4.242239
333.427448	6186.869063	8.194893	-0.065451	4.244920
333.662518	6194.940543	8.199898	-0.065500	4.247648
333.835806	6202.998830	8.204902	-0.065538	4.250369
334.091779	6210.951522	8.209907	-0.065591	4.253054
334.934244	6218.959435	8.214912	-0.065753	4.255761
335.107407	6226.986217	8.219917	-0.065790	4.258467
335.555607	6235.018405	8.224922	-0.065879	4.261175
335.830262	6243.052632	8.229926	-0.065935	4.263880
335.680077	6251.141628	8.234931	-0.065912	4.266598
336.343716	6259.081084	8.239936	-0.066041	4.269271
336.237617	6267.179095	8.244941	-0.066027	4.271989
336.817229	6275.091368	8.249946	-0.066140	4.274649
336.309063	6283.197084	8.254950	-0.066050	4.277362
336.930295	6291.111891	8.259955	-0.066171	4.280020
337.572801	6299.108685	8.264960	-0.066296	4.282704
337.425486	6307.126182	8.269965	-0.066274	4.285386
337.207614	6315.227163	8.274970	-0.066238	4.288094
337.436220	6323.289181	8.279974	-0.066286	4.290790
338.097711	6331.228665	8.284979	-0.066414	4.293448
338.204935	6339.307126	8.289984	-0.066440	4.296146
338.075132	6347.313757	8.294989	-0.066421	4.298816
338.277813	6355.297736	8.299994	-0.066463	4.301480
338.533978	6363.292839	8.304998	-0.066516	4.304146
338.783922	6371.351321	8.310003	-0.066568	4.306831
339.546839	6379.339651	8.315008	-0.066715	4.309496
339.842501	6387.322777	8.320013	-0.066776	4.312154
339.737035	6395.359766	8.325018	-0.066761	4.314824
339.652279	6403.430317	8.330022	-0.066750	4.317504
340.022213	6411.375833	8.335027	-0.066825	4.320145
340.321223	6419.405338	8.340032	-0.066885	4.322811
340.159923	6427.436302	8.345037	-0.066861	4.325472
340.122024	6435.465339	8.350042	-0.066859	4.328132
340.408351	6443.465908	8.355046	-0.066917	4.330783
341.119373	6451.400794	8.360051	-0.067055	4.333415
341.209539	6459.539891	8.365056	-0.067077	4.336107
341.631494	6467.480571	8.370061	-0.067160	4.338735
341.378341	6475.594459	8.375066	-0.067119	4.341413
342.195068	6483.500804	8.380070	-0.067276	4.344030
342.091189	6491.555818	8.385075	-0.067262	4.346686
342.225331	6499.608332	8.390080	-0.067292	4.349342
342.562385	6507.651704	8.395085	-0.067360	4.351995
342.949028	6515.628819	8.400090	-0.067437	4.354624
343.006146	6523.718932	8.405094	-0.067453	4.357287
343.387590	6531.579839	8.410099	-0.067529	4.359875
343.750727	6539.655962	8.415104	-0.067602	4.362532
343.945700	6547.619158	8.420109	-0.067643	4.365150
344.074749	6555.644779	8.425114	-0.067672	4.367785
344.313767	6563.711012	8.430118	-0.067722	4.370433
344.188433	6571.735730	8.435123	-0.067704	4.373064
344.776410	6579.773022	8.440128	-0.067819	4.375701
344.838004	6587.796876	8.445133	-0.067835	4.378329
344.835375	6595.868902	8.450138	-0.067840	4.380971
344.937130	6603.840544	8.455142	-0.067864	4.383579
345.442938	6611.776270	8.460147	-0.067963	4.386177
345.913371	6619.840938	8.465152	-0.068056	4.388815
345.775064	6627.904642	8.470157	-0.068036	4.391446
346.026038	6635.870685	8.475162	-0.068087	4.394047
346.788443	6643.900488	8.480166	-0.068235	4.396671
346.204967	6651.913590	8.485171	-0.068131	4.399279
346.614922	6659.974469	8.490176	-0.068213	4.401907
346.583006	6667.925935	8.495181	-0.068212	4.404495
346.968512	6675.951017	8.500186	-0.068289	4.407108
347.039814	6684.015688	8.505190	-0.068307	4.409731
347.437280	6692.044590	8.510195	-0.068387	4.412342
347.804636	6700.052998	8.515200	-0.068460	4.414945
347.884351	6708.116698	8.520205	-0.068480	4.417562
348.003734	6716.134446	8.525210	-0.068508	4.420163
348.475953	6724.138226	8.530214	-0.068601	4.422760
348.884339	6732.168265	8.535219	-0.068682	4.425364
349.198815	6740.195178	8.540224	-0.068746	4.427965
349.831257	6748.178093	8.545229	-0.068869	4.430551
350.262386	6756.154840	8.550234	-0.068954	4.433133
350.169414	6764.282355	8.555238	-0.068942	4.435760
350.380613	6772.197913	8.560243	-0.068986	4.438317
350.579307	6780.303106	8.565248	-0.069029	4.440935
351.055800	6788.208332	8.570253	-0.069122	4.443488
350.913046	6796.337337	8.575258	-0.069101	4.446108
351.048254	6804.339775	8.580263	-0.069131	4.448687
351.336575	6812.354246	8.585267	-0.069190	4.451270
352.200754	6820.281249	8.590272	-0.069356	4.453826
351.948987	6828.418336	8.595277	-0.069315	4.456442
352.272449	6836.377664	8.600282	-0.069380	4.459002
352.162104	6844.476379	8.605287	-0.069365	4.461604
352.343662	6852.402439	8.610291	-0.069404	4.464150
352.234659	6860.514365	8.615296	-0.069389	4.466753
352.738640	6868.440259	8.620301	-0.069488	4.469297
353.272735	6876.415273	8.625306	-0.069592	4.471856
353.920015	6884.417891	8.630311	-0.069718	4.474422
354.136634	6892.469235	8.635315	-0.069763	4.477001
354.366696	6900.474386	8.640320	-0.069812	4.479564
353.933211	6908.575938	8.645325	-0.069736	4.482153
354.618733	6916.468209	8.650330	-0.069869	4.484678
354.897192	6924.561033	8.655335	-0.069926	4.487265
354.973200	6932.553582	8.660339	-0.069945	4.489816
354.946073	6940.641058	8.665344	-0.069945	4.492397
355.510711	6948.557542	8.670349	-0.070056	4.494923
355.852094	6956.621505	8.675354	-0.070124	4.497495
356.028380	6964.699033	8.680359	-0.070162	4.500068
355.766729	6972.673512	8.685363	-0.070119	4.502606
355.856755	6980.710232	8.690368	-0.070141	4.505163
356.480742	6988.706306	8.695373	-0.070262	4.507708
356.388662	6996.743518	8.700378	-0.070250	4.510261
357.215418	7004.688815	8.705383	-0.070409	4.512788
357.528811	7012.643353	8.710387	-0.070473	4.515314
358.195880	7020.703145	8.715392	-0.070602	4.517873
358.180191	7028.726482	8.720397	-0.070604	4.520417
357.963665	7036.742552	8.725402	-0.070569	4.522956
358.329524	7044.767195	8.730407	-0.070643	4.525499
358.724192	7052.779454	8.735411	-0.070721	4.528036
358.828231	7060.824776	8.740416	-0.070746	4.530581
358.844312	7068.828070	8.745421	-0.070754	4.533112
359.289994	7076.816158	8.750426	-0.070842	4.535637
359.558103	7084.842093	8.755431	-0.070897	4.538173
359.496325	7092.874492	8.760435	-0.070891	4.540708
359.372728	7100.911884	8.765440	-0.070873	4.543243
359.878601	7108.918815	8.770445	-0.070973	4.545768
360.447890	7116.853582	8.775450	-0.071084	4.548270
360.332725	7124.952033	8.780455	-0.071067	4.550820
360.949896	7132.934282	8.785459	-0.071188	4.553334
360.893790	7140.977843	8.790464	-0.071182	4.555864
360.630512	7149.005515	8.795469	-0.071138	4.558387
360.913465	7157.011808	8.800474	-0.071196	4.560904
361.100314	7164.990487	8.805479	-0.071236	4.563410
360.961913	7173.043466	8.810483	-0.071216	4.565937
361.697997	7181.018526	8.815488	-0.071358	4.568440
362.475783	7189.062742	8.820493	-0.071508	4.570964
362.176944	7197.085395	8.825498	-0.071457	4.573477
361.946348	7205.191724	8.830503	-0.071420	4.576015
361.942148	7213.083671	8.835507	-0.071424	4.578485
362.549294	7221.138233	8.840512	-0.071542	4.581006
362.461032	7229.110285	8.845517	-0.071531	4.583498
362.932970	7237.126749	8.850522	-0.071624	4.586004
363.374462	7245.181941	8.855527	-0.071712	4.588520
363.327807	7253.220035	8.860531	-0.071708	4.591029
363.872260	7261.169736	8.865536	-0.071815	4.593510
363.947885	7269.249190	8.870541	-0.071834	4.596029
363.856363	7277.224573	8.875546	-0.071822	4.598514
363.789939	7285.334493	8.880551	-0.071815	4.601040
364.155047	7293.199426	8.885555	-0.071888	4.603488
364.689943	7301.274872	8.890560	-0.071993	4.606001
364.537753	7309.277917	8.895565	-0.071970	4.608489
365.252148	7317.274445	8.900570	-0.072108	4.610975
365.443695	7325.303275	8.905575	-0.072149	4.613469
366.072681	7333.277974	8.910579	-0.072271	4.615945
366.185157	7341.285720	8.915584	-0.072297	4.618430
366.535237	7349.327475	8.920589	-0.072367	4.620923
366.514232	7357.320120	8.925594	-0.072369	4.623400
366.356464	7365.442341	8.930599	-0.072344	4.625916
366.617430	7373.390634	8.935603	-0.072398	4.628377
367.311580	7381.482863	8.940608	-0.072533	4.630881
366.972633	7389.490323	8.945613	-0.072475	4.633357
367.280091	7397.463771	8.950618	-0.072537	4.635822
367.719678	7405.471782	8.955623	-0.072624	4.638295
367.726976	7413.506858	8.960627	-0.072631	4.640776
367.817359	7421.479397	8.965632	-0.072653	4.643236
368.679646	7429.437644	8.970637	-0.072818	4.645691
368.908163	7437.465436	8.975642	-0.072866	4.648165
369.100196	7445.579712	8.980647	-0.072907	4.650665
369.121931	7453.591918	8.985651	-0.072916	4.653132
369.350682	7461.590198	8.990656	-0.072964	4.655594
369.266843	7469.638327	8.995661	-0.072954	4.658069
369.329483	7477.617680	9.000666	-0.072971	4.660522
369.984272	7485.600803	9.005671	-0.073098	4.662975
370.564160	7493.576105	9.010675	-0.073211	4.665423
370.759302	7501.685559	9.015680	-0.073252	4.667912
370.799718	7509.719783	9.020685	-0.073265	4.670377
370.872773	7517.755275	9.025690	-0.073284	4.672840
371.013812	7525.798231	9.030695	-0.073315	4.675305
371.175339	7533.721139	9.035699	-0.073350	4.677731
372.074365	7541.684615	9.040704	-0.073523	4.680168
371.939806	7549.732696	9.045709	-0.073503	4.682631
372.344374	7557.693485	9.050714	-0.073584	4.685065
373.003951	7565.760475	9.055719	-0.073712	4.687529
373.383430	7573.718652	9.060723	-0.073787	4.689960
373.507661	7581.795862	9.065728	-0.073816	4.692426
373.643087	7589.810891	9.070733	-0.073846	4.694871
373.881632	7597.877643	9.075738	-0.073896	4.697331
373.940433	7605.906021	9.080743	-0.073912	4.699778
374.123611	7613.863266	9.085747	-0.073951	4.702202
374.277937	7621.912773	9.090752	-0.073985	4.704653
374.638921	7629.960283	9.095757	-0.074058	4.707101
374.515795	7637.960599	9.100762	-0.074040	4.709535
374.912519	7646.029166	9.105767	-0.074119	4.711987
375.460458	7653.851061	9.110771	-0.074226	4.714363
375.776704	7661.993646	9.115776	-0.074290	4.716835
375.746107	7669.964876	9.120781	-0.074290	4.719255
376.009262	7678.013902	9.125786	-0.074344	4.721696
375.946299	7685.958194	9.130791	-0.074337	4.724105
376.674047	7693.972079	9.135795	-0.074478	4.726533
377.329312	7701.953840	9.140800	-0.074605	4.728949
377.029875	7710.110211	9.145805	-0.074555	4.731419
376.998830	7718.089836	9.150810	-0.074554	4.733833
377.486761	7726.162767	9.155815	-0.074650	4.736274
377.633552	7734.141589	9.160819	-0.074683	4.738685
377.871736	7742.236833	9.165824	-0.074732	4.741130
378.465808	7750.134217	9.170829	-0.074848	4.743514
378.064568	7758.207264	9.175834	-0.074778	4.745951
378.486714	7766.243099	9.180839	-0.074862	4.748374
378.621753	7774.248810	9.185843	-0.074892	4.750787
379.255956	7782.245115	9.190848	-0.075016	4.753195
379.564887	7790.284479	9.195853	-0.075078	4.755616
379.675297	7798.261009	9.200858	-0.075104	4.758017
380.267128	7806.274898	9.205863	-0.075220	4.760426
379.879404	7814.281194	9.210867	-0.075152	4.762835
380.040118	7822.339019	9.215872	-0.075188	4.765256
380.297075	7830.362410	9.220877	-0.075241	4.767666
380.477639	7838.340356	9.225882	-0.075279	4.770061
380.741574	7846.421015	9.230887	-0.075334	4.772485
381.277437	7854.295164	9.235891	-0.075439	4.774845
381.615924	7862.400585	9.240896	-0.075507	4.777274
381.754446	7870.339370	9.245901	-0.075538	4.779653
382.322676	7878.397220	9.250906	-0.075649	4.782064
382.661463	7886.394310	9.255911	-0.075717	4.784457
382.725562	7894.443688	9.260915	-0.075734	4.786865
382.308019	7902.571169	9.265920	-0.075662	4.789296
382.926093	7910.572237	9.270925	-0.075782	4.791686
382.886563	7918.468581	9.275930	-0.075780	4.794045
382.912427	7926.573519	9.280935	-0.075790	4.796465
383.156840	7934.445537	9.285939	-0.075840	4.798813
383.653429	7942.560119	9.290944	-0.075938	4.801232
383.690144	7950.528794	9.295949	-0.075950	4.803607
383.776712	7958.528257	9.300954	-0.075971	4.805990
384.008387	7966.581802	9.305959	-0.076020	4.808388
384.296402	7974.601374	9.310963	-0.076079	4.810774
384.091626	7982.658493	9.315968	-0.076046	4.813172
384.155626	7990.077325	9.320973	-0.076062	4.815378
384.662372	7994.601015	9.325978	-0.076160	4.816721

384.937102	7997.277044	9.330983	-0.076212	4.817515
385.025904	7998.425470	9.335987	-0.076230	4.817856
384.918684	7998.856885	9.340992	-0.076210	4.817985
384.777088	7999.903552	9.345997	-0.076184	4.818296
385.174345	7999.847964	9.351002	-0.076258	4.818278
385.487059	7999.822757	9.356007	-0.076316	4.818270
385.527826	7999.829608	9.361011	-0.076324	4.818271
385.830810	7999.867314	9.366016	-0.076380	4.818281
385.956626	7999.834334	9.371021	-0.076404	4.818271
386.394339	7999.784546	9.376026	-0.076485	4.818255
386.686276	7999.767466	9.381031	-0.076539	4.818248
386.452603	7999.777970	9.386035	-0.076496	4.818252
387.028647	7999.772080	9.391040	-0.076603	4.818248
386.968525	7999.816448	9.396045	-0.076592	4.818262
386.554513	7999.794046	9.401050	-0.076515	4.818257
386.872870	7999.825658	9.406055	-0.076574	4.818265
386.678929	7999.809378	9.411059	-0.076538	4.818261
386.703276	7999.889561	9.416064	-0.076542	4.818285
387.187105	7999.793112	9.421069	-0.076632	4.818254
387.104439	7999.803552	9.426074	-0.076617	4.818257
387.310682	7999.860972	9.431079	-0.076655	4.818274
387.386926	7999.829424	9.436083	-0.076669	4.818264
387.637642	7999.807587	9.441088	-0.076716	4.818256
387.676812	7999.814417	9.446093	-0.076723	4.818258
387.693997	7999.799935	9.451098	-0.076726	4.818254
388.065091	7999.809145	9.456103	-0.076795	4.818255
388.392289	7999.785189	9.461107	-0.076856	4.818247
388.447374	7999.773320	9.466112	-0.076866	4.818243
388.032892	7999.780330	9.471117	-0.076789	4.818247
388.246377	7999.782158	9.476122	-0.076829	4.818246
388.306214	7999.819740	9.481127	-0.076840	4.818257
388.179767	7999.779151	9.486131	-0.076816	4.818246
388.329717	7999.789578	9.491136	-0.076844	4.818248
388.496151	7999.790772	9.496141	-0.076875	4.818248
388.385120	7999.836555	9.501146	-0.076855	4.818262
388.323571	7999.854635	9.506151	-0.076843	4.818268
388.538414	7999.797638	9.511155	-0.076883	4.818250
388.636391	7999.851498	9.516160	-0.076901	4.818265
388.029271	7999.904242	9.521165	-0.076788	4.818284
388.351995	7999.863412	9.526170	-0.076848	4.818270
388.212809	7999.906714	9.531175	-0.076822	4.818284
388.468057	7999.862872	9.536179	-0.076870	4.818270
388.640231	7999.841026	9.541184	-0.076902	4.818262
388.508731	7999.859212	9.546189	-0.076877	4.818268
388.844609	7999.817510	9.551194	-0.076940	4.818255
388.544512	7999.883857	9.556199	-0.076884	4.818275
388.249712	7999.858856	9.561203	-0.076829	4.818269
388.305246	7999.905838	9.566208	-0.076839	4.818283
388.563956	7999.875704	9.571213	-0.076887	4.818273
388.468288	7999.866002	9.576218	-0.076869	4.818270
388.794301	7999.880910	9.581223	-0.076930	4.818274
388.730023	7999.840108	9.586227	-0.076918	4.818262
388.989781	7999.809988	9.591232	-0.076966	4.818252
389.137663	7999.842456	9.596237	-0.076994	4.818261
389.271439	7999.817990	9.601242	-0.077019	4.818253
389.307054	7999.830027	9.606247	-0.077025	4.818256
389.411664	7999.777845	9.611251	-0.077045	4.818241
389.685319	7999.826725	9.616256	-0.077096	4.818254
389.740507	7999.792790	9.621261	-0.077106	4.818244
389.184689	7999.806294	9.626266	-0.077002	4.818250
389.252214	7999.855540	9.631271	-0.077015	4.818264
389.021342	7999.814589	9.636275	-0.076972	4.818253
389.538022	7999.793194	9.641280	-0.077068	4.818245
390.072347	7999.745768	9.646285	-0.077167	4.818228
389.970424	7999.771709	9.651290	-0.077148	4.818236
389.965569	7999.744319	9.656295	-0.077147	4.818228
389.706319	7999.787049	9.661299	-0.077099	4.818242
389.857460	7999.809054	9.666304	-0.077127	4.818248
389.725772	7999.813576	9.671309	-0.077103	4.818250
389.378771	7999.822545	9.676314	-0.077038	4.818254
389.674806	7999.824440	9.681319	-0.077093	4.818253
389.618503	7999.840489	9.686323	-0.077083	4.818258
389.622691	7999.834237	9.691328	-0.077083	4.818256
389.956487	7999.818779	9.696333	-0.077145	4.818251
390.215259	7999.763427	9.701338	-0.077194	4.818233
389.851481	7999.842574	9.706343	-0.077126	4.818258
390.121366	7999.763202	9.711347	-0.077176	4.818233
389.811905	7999.825219	9.716352	-0.077118	4.818253
390.130391	7999.820063	9.721357	-0.077178	4.818250
390.207409	7999.731780	9.726362	-0.077192	4.818224
390.361176	7999.796905	9.731367	-0.077221	4.818242
390.220450	7999.801305	9.736371	-0.077194	4.818244
389.963196	7999.857722	9.741376	-0.077146	4.818262
390.016664	7999.843730	9.746381	-0.077156	4.818258
390.114499	7999.833490	9.751386	-0.077174	4.818254
390.218922	7999.849610	9.756391	-0.077194	4.818259
390.049367	7999.827349	9.761395	-0.077162	4.818253
389.955201	7999.837632	9.766400	-0.077145	4.818256
390.260461	7999.831247	9.771405	-0.077201	4.818253
390.215872	7999.793862	9.776410	-0.077193	4.818242
390.361825	7999.808441	9.781415	-0.077220	4.818246
390.006269	7999.828852	9.786419	-0.077154	4.818253
390.742632	7999.827244	9.791424	-0.077291	4.818250
390.700324	7999.879211	9.796429	-0.077283	4.818265
390.679654	7999.789606	9.801434	-0.077279	4.818239
390.796500	7999.767013	9.806439	-0.077301	4.818232
390.307022	7999.868630	9.811443	-0.077210	4.818264
390.392212	7999.870829	9.816448	-0.077226	4.818264
390.948203	7999.838411	9.821453	-0.077329	4.818252
390.945959	7999.843632	9.826458	-0.077329	4.818254
391.159525	7999.777160	9.831463	-0.077368	4.818233
391.139644	7999.866211	9.836467	-0.077365	4.818260
391.238998	7999.841280	9.841472	-0.077383	4.818252
390.778800	7999.803528	9.846477	-0.077297	4.818243
390.703050	7999.806704	9.851482	-0.077283	4.818244
390.908080	7999.858863	9.856487	-0.077321	4.818259
390.561217	7999.865730	9.861491	-0.077257	4.818262
391.009828	7999.816097	9.866496	-0.077340	4.818246
390.786425	7999.834090	9.871501	-0.077298	4.818252
390.214602	7999.854729	9.876506	-0.077192	4.818260
390.007533	7999.913926	9.881511	-0.077153	4.818279
390.102624	7999.886836	9.886515	-0.077171	4.818270
390.091386	7999.886681	9.891520	-0.077169	4.818270
389.891470	7999.893433	9.896525	-0.077132	4.818273
390.600540	7999.837863	9.901530	-0.077264	4.818254
390.317447	7999.888676	9.906535	-0.077211	4.818270
390.024790	7999.842683	9.911539	-0.077156	4.818257
389.943253	7999.882561	9.916544	-0.077141	4.818270
389.918285	7999.950525	9.921549	-0.077136	4.818290
389.693800	7999.895996	9.926554	-0.077095	4.818275
390.316332	7999.879188	9.931559	-0.077210	4.818267
390.095698	7999.884609	9.936563	-0.077169	4.818270
390.120939	7999.903862	9.941568	-0.077174	4.818275
390.285585	7999.907135	9.946573	-0.077205	4.818275
390.485166	7999.854135	9.951578	-0.077242	4.818259
390.280017	7999.903901	9.956583	-0.077203	4.818275
390.009409	7999.958036	9.961587	-0.077153	4.818292
390.611090	7999.895761	9.966592	-0.077265	4.818271
390.377289	7999.897851	9.971597	-0.077221	4.818272
390.334002	7999.907771	9.976602	-0.077213	4.818275
390.486463	7999.852032	9.981607	-0.077242	4.818258
390.159744	7999.844460	9.986611	-0.077181	4.818257
389.932289	7999.927551	9.991616	-0.077138	4.818283
389.892182	7999.934361	9.996621	-0.077131	4.818285
389.771845	7999.929579	10.001626	-0.077108	4.818284
390.474918	7999.918063	10.006631	-0.077239	4.818278
390.139478	7999.939796	10.011635	-0.077177	4.818286
390.309941	7999.912674	10.016640	-0.077209	4.818277
390.987475	7999.885052	10.021645	-0.077335	4.818266
390.496640	7999.940412	10.026650	-0.077243	4.818285
390.510679	7999.941650	10.031655	-0.077246	4.818285
390.689943	7999.885223	10.036659	-0.077279	4.818267
390.898749	7999.883839	10.041664	-0.077318	4.818266
391.066413	7999.848273	10.046669	-0.077349	4.818255
391.153342	7999.825275	10.051674	-0.077365	4.818248
391.429315	7999.840564	10.056679	-0.077417	4.818251
390.724475	7999.825775	10.061683	-0.077285	4.818250
390.638929	7999.858242	10.066688	-0.077269	4.818260
391.078165	7999.852619	10.071693	-0.077351	4.818256
391.202637	7999.821722	10.076698	-0.077374	4.818246
391.184336	7999.856150	10.081703	-0.077371	4.818257
391.302240	7999.823063	10.086707	-0.077393	4.818246
391.622987	7999.890451	10.091712	-0.077452	4.818265
391.542397	7999.809491	10.096717	-0.077437	4.818241
391.324145	7999.852774	10.101722	-0.077397	4.818255
391.291937	7999.818707	10.106727	-0.077391	4.818245
391.216718	7999.805077	10.111731	-0.077376	4.818241
391.440961	7999.801801	10.116736	-0.077418	4.818240
392.076572	7999.888161	10.121741	-0.077537	4.818263
391.906677	7999.813348	10.126746	-0.077505	4.818241
391.847761	7999.827260	10.131751	-0.077494	4.818246
391.930688	7999.787395	10.136755	-0.077509	4.818233
391.738392	7999.915099	10.141760	-0.077473	4.818272
391.423676	7999.861447	10.146765	-0.077415	4.818257
391.373509	7999.846053	10.151770	-0.077405	4.818253
391.624268	7999.842086	10.156775	-0.077452	4.818251
391.227478	7999.869293	10.161779	-0.077378	4.818261
391.192291	7999.900340	10.166784	-0.077371	4.818270
391.527745	7999.897518	10.171789	-0.077434	4.818268
391.181521	7999.879170	10.176794	-0.077369	4.818264
391.722463	7999.857060	10.181799	-0.077470	4.818255
391.902333	7999.859490	10.186803	-0.077504	4.818255
392.203326	7999.837287	10.191808	-0.077559	4.818247
392.031423	7999.797126	10.196813	-0.077527	4.818236
391.356264	7999.842636	10.201818	-0.077402	4.818252
391.523453	7999.875369	10.206823	-0.077433	4.818261
391.664305	7999.827880	10.211827	-0.077459	4.818246
391.769928	7999.815644	10.216832	-0.077479	4.818242
391.591845	7999.939337	10.221837	-0.077445	4.818280
391.788249	7999.806428	10.226842	-0.077482	4.818240
391.768801	7999.824026	10.231847	-0.077478	4.818245
391.613487	7999.819821	10.236851	-0.077449	4.818244
392.158129	7999.766234	10.241856	-0.077551	4.818226
392.391589	7999.794611	10.246861	-0.077594	4.818234
392.051231	8000.128390	10.251866	-0.077531	4.818334
392.341296	7999.792873	10.256871	-0.077585	4.818233
392.262699	7999.875877	10.261875	-0.077570	4.818258
392.268987	7999.748802	10.266880	-0.077571	4.818221
392.545382	7999.868137	10.271885	-0.077622	4.818255
392.497653	7999.777111	10.276890	-0.077614	4.818228
392.539409	7999.838624	10.281895	-0.077621	4.818246
392.136646	7999.865749	10.286899	-0.077546	4.818256
392.098398	7999.843159	10.291904	-0.077539	4.818249
392.173446	7999.846273	10.296909	-0.077553	4.818250
392.193383	7999.786639	10.301914	-0.077557	4.818232
392.420205	7999.772891	10.306919	-0.077599	4.818227
392.400804	7999.889274	10.311923	-0.077595	4.818262
392.020144	7999.836830	10.316928	-0.077524	4.818248
392.107970	7999.864287	10.321933	-0.077541	4.818256
391.719969	7999.850628	10.326938	-0.077468	4.818253
391.989104	7999.858469	10.331943	-0.077518	4.818254
392.065155	7999.866851	10.336947	-0.077533	4.818256
392.252761	7999.859928	10.341952	-0.077567	4.818254
392.269893	7999.838088	10.346957	-0.077571	4.818247
391.911514	7999.781743	10.351962	-0.077504	4.818232
392.126587	7999.861364	10.356967	-0.077544	4.818255
392.396332	7999.807212	10.361971	-0.077594	4.818237
392.230195	7999.931068	10.366976	-0.077563	4.818275
392.474968	7999.833491	10.371981	-0.077608	4.818245
391.935437	7999.856663	10.376986	-0.077508	4.818254
392.365522	7999.845665	10.381991	-0.077588	4.818249
392.322371	7999.809348	10.386995	-0.077580	4.818238
391.361517	7999.893027	10.392000	-0.077401	4.818267
391.524124	7999.917292	10.397005	-0.077431	4.818274
392.582679	7999.817064	10.402010	-0.077628	4.818240
392.607511	7999.811092	10.407015	-0.077633	4.818238
392.381837	7999.789119	10.412019	-0.077591	4.818232
391.980403	7999.818363	10.417024	-0.077516	4.818242
391.866846	7999.852554	10.422029	-0.077495	4.818253
391.903939	7999.928716	10.427034	-0.077502	4.818275
392.594672	7999.835073	10.432039	-0.077630	4.818245
392.162308	7999.823964	10.437043	-0.077550	4.818243
392.357092	7999.824495	10.442048	-0.077586	4.818243
392.647273	7999.814757	10.447053	-0.077640	4.818239
392.495098	7999.856832	10.452058	-0.077612	4.818252
392.525546	7999.825714	10.457063	-0.077617	4.818242
392.470597	7999.836527	10.462067	-0.077607	4.818246
392.648702	7999.856799	10.467072	-0.077640	4.818251
392.521463	7999.847718	10.472077	-0.077616	4.818249
392.103460	7999.857822	10.477082	-0.077538	4.818254
392.039654	7999.884278	10.482087	-0.077526	4.818262
391.582811	7999.883349	10.487091	-0.077441	4.818263
392.267447	7999.832708	10.492096	-0.077569	4.818246
392.981081	7999.805581	10.497101	-0.077702	4.818235
392.355666	7999.905356	10.502106	-0.077585	4.818267
392.484098	7999.813561	10.507111	-0.077609	4.818239
392.374300	7999.814174	10.512115	-0.077588	4.818240
391.948305	7999.854646	10.517120	-0.077509	4.818253
391.986727	7999.880384	10.522125	-0.077516	4.818261
392.040819	7999.845383	10.527130	-0.077526	4.818250
391.820861	7999.942237	10.532135	-0.077485	4.818280
391.826038	7999.833012	10.537139	-0.077486	4.818247
392.201728	7999.839143	10.542144	-0.077556	4.818248
392.374957	7999.875112	10.547149	-0.077588	4.818258
392.401533	7999.872316	10.552154	-0.077593	4.818257
392.418732	7999.838917	10.557159	-0.077596	4.818247
392.075676	7999.858442	10.562163	-0.077532	4.818254
392.251216	7999.862916	10.567168	-0.077565	4.818255
392.172394	7999.868152	10.572173	-0.077550	4.818256
391.858546	7999.858648	10.577178	-0.077492	4.818255
392.520239	7999.843427	10.582183	-0.077615	4.818248
392.170531	7999.847099	10.587187	-0.077550	4.818250
392.197468	7999.875834	10.592192	-0.077555	4.818259
392.259554	7999.907147	10.597197	-0.077566	4.818268
392.155133	7999.891018	10.602202	-0.077547	4.818263
391.933086	7999.925843	10.607207	-0.077506	4.818275
392.134027	7999.895981	10.612211	-0.077543	4.818265
391.818862	7999.955817	10.617216	-0.077484	4.818284
391.571042	7999.944054	10.622221	-0.077438	4.818281
391.787907	7999.900746	10.627226	-0.077478	4.818268
391.973582	7999.906408	10.632231	-0.077513	4.818269
391.929704	7999.867979	10.637235	-0.077505	4.818257
391.964227	7999.847425	10.642240	-0.077511	4.818251
392.279659	7999.839079	10.647245	-0.077570	4.818247
392.518334	7999.837051	10.652250	-0.077614	4.818246
392.648358	7999.836706	10.657255	-0.077638	4.818245
393.059171	7999.912674	10.662259	-0.077715	4.818266
393.109131	7999.808256	10.667264	-0.077724	4.818235
392.840749	7999.840351	10.672269	-0.077674	4.818246
392.850249	7999.798440	10.677274	-0.077676	4.818233
392.777799	7999.839493	10.682279	-0.077662	4.818246
392.792700	7999.811317	10.687283	-0.077665	4.818237
393.187577	7999.927004	10.692288	-0.077738	4.818270
393.251322	7999.791245	10.697293	-0.077750	4.818229
393.170118	7999.893132	10.702298	-0.077735	4.818260
393.260450	7999.773497	10.707303	-0.077752	4.818224
393.351062	7999.880863	10.712307	-0.077769	4.818256
392.916446	7999.824532	10.717312	-0.077688	4.818241
392.686129	7999.871855	10.722317	-0.077645	4.818256
392.760339	7999.874958	10.727322	-0.077659	4.818256
393.087928	7999.836302	10.732327	-0.077719	4.818243
392.994928	7999.820327	10.737331	-0.077702	4.818239
392.924114	7999.813060	10.742336	-0.077689	4.818237
393.268348	7999.861855	10.747341	-0.077753	4.818250
393.180984	7999.844905	10.752346	-0.077737	4.818246
393.282730	7999.839974	10.757351	-0.077755	4.818244
393.368943	7999.804356	10.762355	-0.077771	4.818233
393.041210	7999.839851	10.767360	-0.077710	4.818245
392.545719	7999.893043	10.772365	-0.077618	4.818262
392.513569	7999.849518	10.777370	-0.077612	4.818250
393.359726	7999.811575	10.782375	-0.077770	4.818235
392.790761	7999.891095	10.787379	-0.077664	4.818261
392.631490	7999.804864	10.792384	-0.077634	4.818236
393.182722	7999.807067	10.797389	-0.077736	4.818234
393.209865	7999.896759	10.802394	-0.077742	4.818261
392.885742	7999.858739	10.807399	-0.077681	4.818251
392.815304	7999.886157	10.812403	-0.077668	4.818259
393.489608	7999.845889	10.817408	-0.077793	4.818245
392.921052	7999.876022	10.822413	-0.077688	4.818256
392.825770	7999.883136	10.827418	-0.077670	4.818258
393.388966	7999.858179	10.832423	-0.077775	4.818249
393.058651	7999.912555	10.837427	-0.077713	4.818266
392.848554	7999.893944	10.842432	-0.077674	4.818261
392.932299	7999.897176	10.847437	-0.077689	4.818262
392.884280	7999.874454	10.852442	-0.077680	4.818256
392.947569	7999.869002	10.857447	-0.077692	4.818254
392.748858	7999.883124	10.862451	-0.077655	4.818259
392.407274	7999.923686	10.867456	-0.077592	4.818272
392.621705	7999.909770	10.872461	-0.077631	4.818267
392.391770	7999.907706	10.877466	-0.077589	4.818267
392.145229	7999.949555	10.882471	-0.077543	4.818281
392.935977	7999.888793	10.887475	-0.077690	4.818260
392.843089	7999.870718	10.892480	-0.077672	4.818255
393.014722	7999.868834	10.897485	-0.077704	4.818253
393.116990	7999.879674	10.902490	-0.077723	4.818256
392.869996	7999.856360	10.907495	-0.077677	4.818250
392.929617	7999.910760	10.912499	-0.077688	4.818266
392.398833	7999.935100	10.917504	-0.077590	4.818275
392.357082	7999.984974	10.922509	-0.077582	4.818290
392.265060	7999.921723	10.927514	-0.077565	4.818272
392.856601	7999.897148	10.932519	-0.077675	4.818262
392.713118	7999.918323	10.937523	-0.077648	4.818269
392.804748	7999.847047	10.942528	-0.077665	4.818248
392.881374	7999.885914	10.947533	-0.077679	4.818259
392.579962	7999.878678	10.952538	-0.077623	4.818258
392.288704	7999.949347	10.957543	-0.077569	4.818280
392.145337	7999.960014	10.962547	-0.077542	4.818284
392.465233	7999.896032	10.967552	-0.077601	4.818264
392.396029	7999.952892	10.972557	-0.077589	4.818281
392.079892	7999.916032	10.977562	-0.077530	4.818271
392.286142	7999.956652	10.982567	-0.077568	4.818282
392.254150	7999.987743	10.987571	-0.077562	4.818292
392.737880	7999.919673	10.992576	-0.077652	4.818270
392.915402	7999.911564	10.997581	-0.077685	4.818266
392.934893	7999.904468	11.002586	-0.077689	4.818264
392.566089	8000.035040	11.007591	-0.077620	4.818305
392.804725	7999.954194	11.012595	-0.077664	4.818280
392.567149	7999.957281	11.017600	-0.077620	4.818281
392.675453	7999.972405	11.022605	-0.077640	4.818285
392.005738	7999.989610	11.027610	-0.077515	4.818293
392.256062	7999.975130	11.032615	-0.077562	4.818288
392.543607	7999.932779	11.037619	-0.077615	4.818274
392.235931	7999.933866	11.042624	-0.077558	4.818276
392.238775	7999.982242	11.047629	-0.077559	4.818290
392.299683	7999.908450	11.052634	-0.077570	4.818268
392.429366	7999.945932	11.057639	-0.077594	4.818279
392.758095	7999.955633	11.062643	-0.077655	4.818280
392.893308	7999.910169	11.067648	-0.077680	4.818266
393.340377	7999.926728	11.072653	-0.077764	4.818269
393.332490	7999.882479	11.077658	-0.077762	4.818256
392.694760	7999.990494	11.082663	-0.077643	4.818291
393.159204	7999.908501	11.087667	-0.077730	4.818265
392.981000	7999.887169	11.092672	-0.077696	4.818259
392.585024	7999.936453	11.097677	-0.077623	4.818275
392.938903	7999.893950	11.102682	-0.077688	4.818261
393.109619	7999.899410	11.107687	-0.077720	4.818262
393.683586	7999.880905	11.112691	-0.077827	4.818254
393.240843	7999.855991	11.117696	-0.077745	4.818249
392.999224	7999.906313	11.122701	-0.077700	4.818265
393.011922	7999.886515	11.127706	-0.077702	4.818259
393.316991	7999.874878	11.132711	-0.077759	4.818254
393.328092	7999.884483	11.137715	-0.077761	4.818257
392.881665	7999.894200	11.142720	-0.077677	4.818261
392.829579	7999.955495	11.147725	-0.077668	4.818280
393.301514	7999.858892	11.152730	-0.077756	4.818249
393.270768	7999.871083	11.157735	-0.077750	4.818253
393.221807	7999.877774	11.162739	-0.077741	4.818255
393.449432	7999.844070	11.167744	-0.077783	4.818244
393.781669	7999.869584	11.172749	-0.077845	4.818251
393.624907	7999.814912	11.177754	-0.077815	4.818235
393.272457	7999.883701	11.182759	-0.077750	4.818257
393.173860	7999.947520	11.187763	-0.077732	4.818276
392.676203	7999.900845	11.192768	-0.077639	4.818264
392.568393	7999.917248	11.197773	-0.077619	4.818270
392.646030	7999.914092	11.202778	-0.077633	4.818268
393.177747	7999.870843	11.207783	-0.077732	4.818253
393.248942	7999.844480	11.212787	-0.077745	4.818245
393.148890	7999.859937	11.217792	-0.077727	4.818250
393.267997	7999.902532	11.222797	-0.077749	4.818262
393.222308	7999.872484	11.227802	-0.077740	4.818254
392.912980	7999.911381	11.232807	-0.077683	4.818266
392.813137	7999.926841	11.237811	-0.077664	4.818271
393.388032	7999.860005	11.242816	-0.077771	4.818249
393.172007	7999.895961	11.247821	-0.077731	4.818261
393.056724	7999.876532	11.252826	-0.077709	4.818256
393.469788	7999.848492	11.257831	-0.077786	4.818246
393.588844	7999.860610	11.262835	-0.077808	4.818249
393.542781	7999.840015	11.267840	-0.077799	4.818243
393.537816	7999.896695	11.272845	-0.077798	4.818260
393.167594	7999.870660	11.277850	-0.077729	4.818253
392.946071	7999.905491	11.282855	-0.077688	4.818265
393.589562	7999.843789	11.287859	-0.077808	4.818244
393.543671	7999.871539	11.292864	-0.077799	4.818252
393.279768	7999.896337	11.297869	-0.077750	4.818261
393.227696	7999.886171	11.302874	-0.077740	4.818258
393.370608	7999.878644	11.307879	-0.077767	4.818255
393.224833	7999.918704	11.312883	-0.077740	4.818267
393.223349	7999.878746	11.317888	-0.077740	4.818256
393.217810	7999.919654	11.322893	-0.077738	4.818268
393.471441	7999.888404	11.327898	-0.077786	4.818257
393.228132	7999.897718	11.332903	-0.077740	4.818261
392.704534	7999.934765	11.337907	-0.077643	4.818274
393.602428	7999.875455	11.342912	-0.077810	4.818253
393.764788	7999.955419	11.347917	-0.077840	4.818276
393.309075	7999.878833	11.352922	-0.077755	4.818255
393.426732	7999.894085	11.357927	-0.077777	4.818259
393.410292	7999.883350	11.362931	-0.077774	4.818256
393.656598	7999.826779	11.367936	-0.077820	4.818238
393.605609	7999.903854	11.372941	-0.077810	4.818261
393.468773	7999.882030	11.377946	-0.077785	4.818256
393.508776	7999.860499	11.382951	-0.077792	4.818249
393.912302	7999.877521	11.387955	-0.077867	4.818252
393.268859	7999.881416	11.392960	-0.077747	4.818256
393.660267	7999.895120	11.397965	-0.077820	4.818259
393.348193	7999.895095	11.402970	-0.077762	4.818260
393.438079	7999.933091	11.407975	-0.077779	4.818271
393.911592	7999.886953	11.412979	-0.077867	4.818255
393.821350	7999.861557	11.417984	-0.077850	4.818248
393.800180	7999.862318	11.422989	-0.077846	4.818248
393.614165	7999.894476	11.427994	-0.077811	4.818259
393.772717	7999.879805	11.432999	-0.077841	4.818254
393.899182	7999.871005	11.438003	-0.077864	4.818251
393.955703	7999.830781	11.443008	-0.077875	4.818238
393.823595	7999.880485	11.448013	-0.077850	4.818254
393.717187	7999.825443	11.453018	-0.077830	4.818238
393.401383	7999.903136	11.458023	-0.077771	4.818262
393.685404	7999.887011	11.463027	-0.077824	4.818256
393.311062	7999.915569	11.468032	-0.077755	4.818266
393.732127	7999.899198	11.473037	-0.077833	4.818260
393.204052	7999.913062	11.478042	-0.077735	4.818266
392.887676	7999.997053	11.483047	-0.077676	4.818292
393.068745	7999.956414	11.488051	-0.077709	4.818279
393.557553	7999.896821	11.493056	-0.077800	4.818260
393.238559	7999.950299	11.498061	-0.077741	4.818277
393.122284	7999.974994	11.503066	-0.077719	4.818285
393.329651	7999.935762	11.508071	-0.077758	4.818272
393.615203	7999.863959	11.513075	-0.077811	4.818250
393.510464	7999.863589	11.518080	-0.077791	4.818250
392.858846	7999.965109	11.523085	-0.077670	4.818283
393.034284	7999.953820	11.528090	-0.077703	4.818279
393.262621	7999.933788	11.533095	-0.077745	4.818272
393.074364	7999.970119	11.538099	-0.077710	4.818283
392.936849	7999.970356	11.543104	-0.077684	4.818284
392.591132	8000.113851	11.548109	-0.077620	4.818328
392.647680	8000.035795	11.553114	-0.077630	4.818305
393.068038	8000.012058	11.558119	-0.077709	4.818296
392.806948	8000.026385	11.563123	-0.077660	4.818301
393.294472	7999.884803	11.568128	-0.077751	4.818257
393.024092	7999.941042	11.573133	-0.077700	4.818275
393.527432	7999.869034	11.578138	-0.077794	4.818251
393.165374	7999.920879	11.583143	-0.077726	4.818268
393.071548	7999.976355	11.588147	-0.077709	4.818285
393.182205	7999.917948	11.593152	-0.077729	4.818267
393.402954	7999.925137	11.598157	-0.077771	4.818269
393.330029	7999.922044	11.603162	-0.077757	4.818268
393.227536	7999.916450	11.608167	-0.077738	4.818267
393.601071	7999.879467	11.613171	-0.077807	4.818254
393.210167	7999.879426	11.618176	-0.077734	4.818256
393.835357	7999.881583	11.623181	-0.077851	4.818254
393.715779	7999.876807	11.628186	-0.077828	4.818253
393.940239	7999.856723	11.633191	-0.077870	4.818246
393.896045	7999.908668	11.638195	-0.077862	4.818262
393.986104	7999.852083	11.643200	-0.077879	4.818245
393.873823	7999.888393	11.648205	-0.077858	4.818256
393.203699	7999.954982	11.653210	-0.077733	4.818278
393.414123	7999.910537	11.658215	-0.077772	4.818264
393.688426	7999.908993	11.663219	-0.077823	4.818263
393.731598	7999.880149	11.668224	-0.077831	4.818254
393.359304	7999.922396	11.673229	-0.077762	4.818268
393.265052	7999.942135	11.678234	-0.077744	4.818274
393.231778	7999.920663	11.683239	-0.077738	4.818268
393.211261	7999.959266	11.688243	-0.077734	4.818280
393.022594	7999.948301	11.693248	-0.077699	4.818277
393.794123	7999.929319	11.698253	-0.077842	4.818268
393.339226	7999.971498	11.703258	-0.077758	4.818283
393.286183	7999.931893	11.708263	-0.077748	4.818271
393.084567	7999.982756	11.713267	-0.077710	4.818287
393.268339	7999.910626	11.718272	-0.077744	4.818265
393.131417	7999.943450	11.723277	-0.077719	4.818275
393.324648	7999.946063	11.728282	-0.077755	4.818275
393.606099	7999.938310	11.733287	-0.077807	4.818272
393.881058	7999.898943	11.738291	-0.077858	4.818259
393.790046	7999.898758	11.743296	-0.077841	4.818259
393.990691	7999.916185	11.748301	-0.077879	4.818264
394.037416	7999.905255	11.753306	-0.077887	4.818260
393.552026	7999.901831	11.758311	-0.077797	4.818261
393.958916	7999.893676	11.763315	-0.077873	4.818257
394.184689	7999.872559	11.768320	-0.077915	4.818250
394.238170	7999.892197	11.773325	-0.077924	4.818256
394.415178	7999.844146	11.778330	-0.077957	4.818241
393.960938	7999.870570	11.783335	-0.077873	4.818250
394.032288	7999.912519	11.788339	-0.077886	4.818262
393.856844	7999.866001	11.793344	-0.077853	4.818249
393.742348	7999.921197	11.798349	-0.077832	4.818266
393.950691	7999.872520	11.803354	-0.077871	4.818251
393.666908	7999.888641	11.808359	-0.077818	4.818257
393.830979	7999.913980	11.813363	-0.077848	4.818264
393.934904	7999.870195	11.818368	-0.077868	4.818250
393.832488	7999.902434	11.823373	-0.077849	4.818260
393.440782	7999.944418	11.828378	-0.077776	4.818274
393.966510	7999.957841	11.833383	-0.077873	4.818276
393.747609	7999.917039	11.838387	-0.077833	4.818265
393.947372	7999.827259	11.843392	-0.077870	4.818237
394.239136	7999.866939	11.848397	-0.077924	4.818248
393.740675	7999.885408	11.853402	-0.077831	4.818256
393.874390	7999.886164	11.858407	-0.077856	4.818255
393.933710	7999.921645	11.863411	-0.077867	4.818265
393.922999	7999.905733	11.868416	-0.077865	4.818261
394.076503	7999.896249	11.873421	-0.077894	4.818257
394.034173	7999.894621	11.878426	-0.077886	4.818257
394.221898	7999.890855	11.883431	-0.077920	4.818255
393.982018	7999.923335	11.888435	-0.077876	4.818266
393.625625	7999.898537	11.893440	-0.077809	4.818260
393.561988	7999.996459	11.898445	-0.077798	4.818289
394.126426	7999.908466	11.903450	-0.077903	4.818261
393.873054	7999.880860	11.908455	-0.077855	4.818254
394.073394	7999.865704	11.913459	-0.077893	4.818248
393.901326	7999.872829	11.918464	-0.077860	4.818251
393.712856	7999.910208	11.923469	-0.077825	4.818263
393.995716	7999.874101	11.928474	-0.077878	4.818251
393.869792	7999.893411	11.933479	-0.077854	4.818257
394.145401	7999.900293	11.938483	-0.077906	4.818258
393.795001	7999.885035	11.943488	-0.077840	4.818255
393.769394	7999.925671	11.948493	-0.077836	4.818267
393.637397	7999.951204	11.953498	-0.077811	4.818275
393.459462	7999.913060	11.958503	-0.077778	4.818265
393.426205	8000.006139	11.963507	-0.077772	4.818293
393.502505	7999.920993	11.968512	-0.077786	4.818267
393.264854	7999.975573	11.973517	-0.077742	4.818284
393.431198	7999.965211	11.978522	-0.077772	4.818280
393.280933	7999.977886	11.983527	-0.077744	4.818285
393.724573	7999.963923	11.988531	-0.077827	4.818279
393.588084	7999.910576	11.993536	-0.077802	4.818264
393.507703	7999.942063	11.998541	-0.077787	4.818273
393.642118	7999.952287	12.003546	-0.077812	4.818276
393.619962	7999.935169	12.008551	-0.077807	4.818271
394.079304	7999.903553	12.013555	-0.077893	4.818260
393.803248	7999.905066	12.018560	-0.077841	4.818261
393.520086	7999.923298	12.023565	-0.077789	4.818268
393.389716	7999.940446	12.028570	-0.077764	4.818273
393.202181	7999.957871	12.033575	-0.077729	4.818279
393.590367	7999.918985	12.038579	-0.077802	4.818266
393.637189	7999.902801	12.043584	-0.077810	4.818261
393.821172	7999.905290	12.048589	-0.077844	4.818261
393.980450	7999.892730	12.053594	-0.077874	4.818257
393.931204	7999.898366	12.058599	-0.077865	4.818259
393.869199	7999.926949	12.063603	-0.077853	4.818267
393.479266	7999.963702	12.068608	-0.077781	4.818280
393.423351	7999.973451	12.073613	-0.077770	4.818283
393.147602	7999.977071	12.078618	-0.077719	4.818285
393.404343	7999.940609	12.083623	-0.077767	4.818273
393.716770	7999.937480	12.088627	-0.077825	4.818271
393.971945	7999.869469	12.093632	-0.077872	4.818250
393.813640	7999.918818	12.098637	-0.077843	4.818265
393.687224	7999.959140	12.103642	-0.077819	4.818278
393.592468	7999.935784	12.108647	-0.077801	4.818271
393.703153	7999.959349	12.113651	-0.077822	4.818278
394.308100	7999.884515	12.118656	-0.077934	4.818253
393.780003	7999.964587	12.123661	-0.077836	4.818279
393.813698	7999.986059	12.128666	-0.077842	4.818285
393.535135	7999.992792	12.133671	-0.077790	4.818288
394.113406	7999.934412	12.138675	-0.077898	4.818269
393.691964	7999.946567	12.143680	-0.077820	4.818274
394.404789	7999.918385	12.148685	-0.077952	4.818263
394.320465	7999.908832	12.153690	-0.077936	4.818260
394.536466	7999.872870	12.158695	-0.077977	4.818249
394.438850	7999.888360	12.163699	-0.077958	4.818254
394.200020	7999.897733	12.168704	-0.077914	4.818257
394.350778	7999.909230	12.173709	-0.077942	4.818260
394.097916	7999.945737	12.178714	-0.077895	4.818272
393.919468	7999.911789	12.183719	-0.077862	4.818263
394.458185	7999.911726	12.188723	-0.077962	4.818261
394.161340	7999.924517	12.193728	-0.077907	4.818265
394.189617	7999.944865	12.198733	-0.077912	4.818271
394.167466	7999.941409	12.203738	-0.077908	4.818270
394.552498	7999.905634	12.208743	-0.077979	4.818258
394.551728	7999.908774	12.213747	-0.077979	4.818259
394.315820	7999.899269	12.218752	-0.077935	4.818257
394.717620	7999.900505	12.223757	-0.078010	4.818256
393.990334	7999.958961	12.228762	-0.077874	4.818276
393.945290	7999.939431	12.233767	-0.077866	4.818271
393.974672	7999.995525	12.238771	-0.077871	4.818287
393.639496	7999.994135	12.243776	-0.077809	4.818288
393.601461	8000.030399	12.248781	-0.077802	4.818299
393.812748	7999.963896	12.253786	-0.077841	4.818279
394.105948	7999.915318	12.258791	-0.077896	4.818263
393.740534	7999.982880	12.263795	-0.077828	4.818285
393.464723	7999.959173	12.268800	-0.077776	4.818279
393.529466	7999.994728	12.273805	-0.077788	4.818289
393.700183	7999.954999	12.278810	-0.077820	4.818276
393.229524	8000.076835	12.283815	-0.077732	4.818315
393.403283	8000.088644	12.288819	-0.077765	4.818317
393.271873	8000.051129	12.293824	-0.077740	4.818307
393.450966	8000.013616	12.298829	-0.077773	4.818295
393.909106	7999.958864	12.303834	-0.077859	4.818277
393.638247	7999.949938	12.308839	-0.077808	4.818275
393.195597	8000.085815	12.313843	-0.077726	4.818317
393.470915	7999.981295	12.318848	-0.077777	4.818285
393.446906	8000.067143	12.323853	-0.077772	4.818311
393.856355	7999.986508	12.328858	-0.077849	4.818285
393.623518	7999.967588	12.333863	-0.077805	4.818280
393.707149	8000.048588	12.338867	-0.077821	4.818304
393.377286	8000.018895	12.343872	-0.077759	4.818297
393.366988	7999.967257	12.348877	-0.077757	4.818281
393.432253	7999.966036	12.353882	-0.077769	4.818281
393.592803	7999.994480	12.358887	-0.077799	4.818289
393.611467	7999.998933	12.363891	-0.077803	4.818290
393.659846	7999.986974	12.368896	-0.077812	4.818286
393.470069	8000.008572	12.373901	-0.077776	4.818293
393.805018	7999.947948	12.378906	-0.077839	4.818274
393.661651	7999.965970	12.383911	-0.077812	4.818280
393.719847	8000.030862	12.388915	-0.077823	4.818299
393.846631	7999.975826	12.393920	-0.077846	4.818282
393.841389	7999.991516	12.398925	-0.077845	4.818287
393.647581	7999.997295	12.403930	-0.077809	4.818289
393.699937	7999.964371	12.408935	-0.077819	4.818279
393.446437	8000.040805	12.413939	-0.077772	4.818303
393.679606	7999.972497	12.418944	-0.077815	4.818282
393.306463	8000.025241	12.423949	-0.077745	4.818299
393.353884	8000.024829	12.428954	-0.077754	4.818299
393.401332	8000.024418	12.433959	-0.077763	4.818298
393.909986	8000.020794	12.438963	-0.077858	4.818295
393.563986	8000.005595	12.443968	-0.077793	4.818292
393.653278	8000.011005	12.448973	-0.077810	4.818293
393.869632	7999.993965	12.453978	-0.077850	4.818287
393.869882	7999.907788	12.458983	-0.077850	4.818262
393.562774	8000.023432	12.463987	-0.077793	4.818297
393.566648	7999.949916	12.468992	-0.077793	4.818275
394.038930	7999.903763	12.473997	-0.077881	4.818260
393.844480	7999.995710	12.479002	-0.077845	4.818288
393.520972	7999.976612	12.484007	-0.077785	4.818284
393.877167	7999.990892	12.489011	-0.077851	4.818286
393.969773	7999.955360	12.494016	-0.077868	4.818275
393.875566	7999.969845	12.499021	-0.077851	4.818280
393.997392	7999.984103	12.504026	-0.077873	4.818284
394.024034	7999.962391	12.509031	-0.077878	4.818277
393.786478	8000.004360	12.514035	-0.077834	4.818291
393.512952	7999.941801	12.519040	-0.077783	4.818273
393.771288	7999.973671	12.524045	-0.077831	4.818282
394.132387	8000.009036	12.529050	-0.077898	4.818291
393.693489	7999.993630	12.534055	-0.077816	4.818288
394.161163	7999.991554	12.539059	-0.077903	4.818285
393.696978	7999.985263	12.544064	-0.077817	4.818285
393.987560	7999.980788	12.549069	-0.077871	4.818283
394.025925	7999.978152	12.554074	-0.077878	4.818282
393.743213	8000.017408	12.559079	-0.077825	4.818295
393.952368	8000.021288	12.564083	-0.077864	4.818295
393.998947	7999.969369	12.569088	-0.077873	4.818280
393.778069	8000.022074	12.574093	-0.077832	4.818296
394.187590	7999.965612	12.579098	-0.077908	4.818278
393.950240	7999.926662	12.584103	-0.077864	4.818267
393.642710	8000.005518	12.589107	-0.077807	4.818292
393.484464	8000.030696	12.594112	-0.077777	4.818300
393.867382	8000.014860	12.599117	-0.077848	4.818294
394.215433	7999.938649	12.604122	-0.077913	4.818270
394.012313	7999.940098	12.609127	-0.077875	4.818271
393.979984	8000.015325	12.614131	-0.077869	4.818293
394.404269	7999.894956	12.619136	-0.077948	4.818256
394.793660	7999.908636	12.624141	-0.078020	4.818258
394.308274	7999.978776	12.629146	-0.077930	4.818281
394.556614	7999.887552	12.634151	-0.077976	4.818253
395.036033	7999.898248	12.639155	-0.078065	4.818254
394.474089	7999.910599	12.644160	-0.077961	4.818260
394.549026	7999.930528	12.649165	-0.077975	4.818266
393.741698	8000.065669	12.654170	-0.077824	4.818309
394.231244	7999.967203	12.659175	-0.077915	4.818278
394.105727	7999.960245	12.664179	-0.077892	4.818276
394.091767	7999.929576	12.669184	-0.077889	4.818267
394.389737	7999.925201	12.674189	-0.077945	4.818265
395.080434	7999.916690	12.679194	-0.078073	4.818260
394.532230	7999.895597	12.684199	-0.077971	4.818256
394.302351	7999.945027	12.689203	-0.077928	4.818271
394.572264	7999.895082	12.694208	-0.077979	4.818255
394.619382	7999.891513	12.699213	-0.077987	4.818254
394.047500	7999.936310	12.704218	-0.077881	4.818270
394.407439	7999.891788	12.709223	-0.077948	4.818255
394.549276	7999.929439	12.714227	-0.077974	4.818265
393.895034	7999.972069	12.719232	-0.077852	4.818281
394.055955	7999.954278	12.724237	-0.077882	4.818275
394.314079	7999.949364	12.729242	-0.077930	4.818272
394.161489	7999.937835	12.734247	-0.077902	4.818270
394.440128	7999.924791	12.739251	-0.077954	4.818265
393.977748	7999.934289	12.744256	-0.077867	4.818269
393.994606	7999.960788	12.749261	-0.077871	4.818277
394.180078	7999.956991	12.754266	-0.077905	4.818275
394.137599	7999.953260	12.759271	-0.077897	4.818274
394.323131	7999.954719	12.764275	-0.077932	4.818274
394.263924	7999.917130	12.769280	-0.077921	4.818263
394.828336	7999.896398	12.774285	-0.078026	4.818255
394.759140	7999.920680	12.779290	-0.078013	4.818262
394.838134	7999.881811	12.784295	-0.078027	4.818250
395.018608	7999.906323	12.789299	-0.078061	4.818257
394.985983	7999.849126	12.794304	-0.078055	4.818240
395.119255	7999.841470	12.799309	-0.078079	4.818237
394.491728	7999.975894	12.804314	-0.077963	4.818280
394.446404	7999.909067	12.809319	-0.077954	4.818260
395.370706	7999.864836	12.814323	-0.078126	4.818243
395.072491	7999.872352	12.819328	-0.078071	4.818246
394.468469	7999.923019	12.824333	-0.077958	4.818264
394.601780	7999.934280	12.829338	-0.077983	4.818267
394.418846	7999.917085	12.834343	-0.077949	4.818262
393.991471	7999.970146	12.839347	-0.077869	4.818280
393.722788	8000.050578	12.844352	-0.077819	4.818305
393.779122	8000.071306	12.849357	-0.077830	4.818311
393.753802	8000.082520	12.854362	-0.077825	4.818314
393.722165	8000.094700	12.859367	-0.077819	4.818318
394.095981	7999.999921	12.864371	-0.077888	4.818288
393.898472	8000.015108	12.869376	-0.077852	4.818294
393.783495	7999.983070	12.874381	-0.077830	4.818285
393.827396	8000.053024	12.879386	-0.077838	4.818305
394.461549	7999.927090	12.884391	-0.077956	4.818265
393.937957	8000.067126	12.889395	-0.077859	4.818309
393.993713	8000.013229	12.894400	-0.077869	4.818293
394.636923	7999.949425	12.899405	-0.077989	4.818271
394.382817	7999.966998	12.904410	-0.077942	4.818277
394.008753	7999.953520	12.909415	-0.077872	4.818275
394.559409	7999.948365	12.914419	-0.077974	4.818271
394.403841	7999.956764	12.919424	-0.077945	4.818274
394.461525	7999.913402	12.924429	-0.077956	4.818261
394.590882	7999.894132	12.929434	-0.077980	4.818255
394.536343	7999.930174	12.934439	-0.077970	4.818266
394.963429	7999.900224	12.939443	-0.078049	4.818255
394.747947	7999.893098	12.944448	-0.078009	4.818254
395.076616	7999.897548	12.949453	-0.078070	4.818254
395.247077	7999.878835	12.954458	-0.078102	4.818248
394.525010	7999.920545	12.959463	-0.077967	4.818263
394.974562	7999.953958	12.964467	-0.078051	4.818271
394.451773	7999.932158	12.969472	-0.077954	4.818267
394.214742	7999.981491	12.974477	-0.077910	4.818282
394.420869	7999.982179	12.979482	-0.077948	4.818282
394.456557	7999.913296	12.984487	-0.077955	4.818261
394.096215	7999.998793	12.989491	-0.077887	4.818288
393.880774	7999.980107	12.994496	-0.077847	4.818283
394.023232	7999.997798	12.999501	-0.077874	4.818288
393.922640	8000.069998	13.004506	-0.077855	4.818310
394.303889	7999.917518	13.009511	-0.077926	4.818263
393.965245	7999.993850	13.014515	-0.077863	4.818287
394.131884	7999.974034	13.019520	-0.077894	4.818280
393.797463	8000.004182	13.024525	-0.077831	4.818291
394.377635	7999.948981	13.029530	-0.077939	4.818272
394.485303	7999.898941	13.034535	-0.077959	4.818257
394.070376	8000.011022	13.039539	-0.077882	4.818292
394.176517	7999.963062	13.044544	-0.077902	4.818277
394.306180	7999.998446	13.049549	-0.077926	4.818287
393.917957	8000.085666	13.054554	-0.077854	4.818315
393.630230	8000.113294	13.059559	-0.077800	4.818324
393.900583	8000.102240	13.064563	-0.077850	4.818320
393.978885	8000.066514	13.069568	-0.077865	4.818309
394.130005	8000.049641	13.074573	-0.077893	4.818303
393.999150	8000.085699	13.079578	-0.077869	4.818314
394.066598	7999.984669	13.084583	-0.077881	4.818284
394.481068	8000.011299	13.089587	-0.077958	4.818290
394.362897	8000.001287	13.094592	-0.077936	4.818288
394.620507	7999.911240	13.099597	-0.077984	4.818260
394.527495	7999.936250	13.104602	-0.077967	4.818268
394.504352	7999.924373	13.109607	-0.077962	4.818264
394.543347	7999.958529	13.114611	-0.077970	4.818274
394.711716	7999.886189	13.119616	-0.078001	4.818252
394.953766	7999.877905	13.124621	-0.078046	4.818249
394.641190	7999.931469	13.129626	-0.077988	4.818266
394.255956	7999.943062	13.134631	-0.077916	4.818271
394.471816	7999.977512	13.139635	-0.077956	4.818280
394.648891	7999.925258	13.144640	-0.077989	4.818264
394.845442	7999.892185	13.149645	-0.078025	4.818253
394.515634	7999.966535	13.154650	-0.077964	4.818277
394.799087	7999.903111	13.159655	-0.078017	4.818257
394.810835	7999.900115	13.164659	-0.078019	4.818256
395.267870	7999.831686	13.169664	-0.078104	4.818234
395.319448	7999.818719	13.174669	-0.078113	4.818230
395.157720	7999.887990	13.179674	-0.078083	4.818251
394.558971	7999.936626	13.184679	-0.077972	4.818268
394.909003	7999.945569	13.189683	-0.078037	4.818269
395.268575	7999.848495	13.194688	-0.078104	4.818239
394.807716	7999.902152	13.199693	-0.078018	4.818256
395.103986	7999.934539	13.204698	-0.078073	4.818265
395.342364	7999.867352	13.209703	-0.078117	4.818244
395.133853	7999.897103	13.214707	-0.078079	4.818254
394.766143	7999.924697	13.219712	-0.078010	4.818263
394.956263	7999.925168	13.224717	-0.078045	4.818263
394.975260	7999.924371	13.229722	-0.078049	4.818262
394.798103	7999.948241	13.234727	-0.078016	4.818270
394.723167	7999.973496	13.239731	-0.078002	4.818278
394.542657	7999.937417	13.244736	-0.077968	4.818268
394.864202	7999.903936	13.249741	-0.078028	4.818257
395.024382	7999.895594	13.254746	-0.078058	4.818254
395.033228	7999.861029	13.259751	-0.078059	4.818243
394.574351	7999.932579	13.264755	-0.077974	4.818266
394.679006	8000.002305	13.269760	-0.077993	4.818287
394.608442	7999.930932	13.274765	-0.077980	4.818266
394.637215	7999.989121	13.279770	-0.077986	4.818283
394.506951	7999.961079	13.284775	-0.077961	4.818275
394.844896	7999.942534	13.289779	-0.078024	4.818268
394.465129	7999.926876	13.294784	-0.077953	4.818265
394.615520	7999.938369	13.299789	-0.077981	4.818268
395.148213	7999.952941	13.304794	-0.078080	4.818270
395.416534	7999.864089	13.309799	-0.078130	4.818243
394.964687	7999.917867	13.314803	-0.078046	4.818261
394.597112	7999.966482	13.319808	-0.077978	4.818276
394.509409	7999.904336	13.324813	-0.077961	4.818258
394.736192	7999.924220	13.329818	-0.078004	4.818263
394.715712	7999.892411	13.334823	-0.078000	4.818254
394.851809	7999.931035	13.339827	-0.078025	4.818265
394.316752	7999.971076	13.344832	-0.077925	4.818279
394.706278	7999.916446	13.349837	-0.077998	4.818261
394.538213	7999.977222	13.354842	-0.077966	4.818280
394.252189	8000.012229	13.359847	-0.077913	4.818291
394.406392	7999.997500	13.364851	-0.077942	4.818286
394.265923	8000.033428	13.369856	-0.077916	4.818298
394.182835	8000.052267	13.374861	-0.077900	4.818304
394.243454	8000.023658	13.379866	-0.077911	4.818295
393.923024	8000.030875	13.384871	-0.077852	4.818298
393.841832	8000.136968	13.389875	-0.077837	4.818330
393.646003	8000.151126	13.394880	-0.077800	4.818335
393.452556	8000.135892	13.399885	-0.077764	4.818331
394.050504	8000.054659	13.404890	-0.077875	4.818305
393.946134	8000.023815	13.409895	-0.077856	4.818296
394.038116	8000.016650	13.414899	-0.077873	4.818294
394.161757	7999.968928	13.419904	-0.077896	4.818279
394.123020	8000.033558	13.424909	-0.077889	4.818298
394.504798	7999.976722	13.429914	-0.077960	4.818280
394.522494	7999.981162	13.434919	-0.077963	4.818281
394.420379	8000.047036	13.439923	-0.077944	4.818301
394.562123	7999.969081	13.444928	-0.077970	4.818277
394.536076	7999.956113	13.449933	-0.077965	4.818274
394.670224	8000.005221	13.454938	-0.077990	4.818288
393.979503	8000.095699	13.459943	-0.077862	4.818317
394.208880	8000.122976	13.464947	-0.077904	4.818325
394.316393	8000.057168	13.469952	-0.077924	4.818305
394.124013	8000.036693	13.474957	-0.077888	4.818299
393.952695	8000.151023	13.479962	-0.077856	4.818334
394.039001	8000.096489	13.484967	-0.077872	4.818317
394.035349	8000.084876	13.489971	-0.077872	4.818314
393.819477	8000.129241	13.494976	-0.077832	4.818328
393.871777	8000.104723	13.499981	-0.077841	4.818320
394.380178	8000.053806	13.504986	-0.077936	4.818303
394.548001	8000.002478	13.509991	-0.077967	4.818287
394.574609	8000.028059	13.514995	-0.077972	4.818295
394.145272	8000.072684	13.520000	-0.077892	4.818310
394.554056	8000.017264	13.525005	-0.077968	4.818292
394.528646	8000.076821	13.530010	-0.077963	4.818310
394.442336	7999.968451	13.535015	-0.077947	4.818278
393.957584	8000.126879	13.540019	-0.077857	4.818327
394.599015	7999.972670	13.545024	-0.077976	4.818278
394.588792	7999.989343	13.550029	-0.077974	4.818283
394.621152	8000.018154	13.555034	-0.077980	4.818292
394.544307	7999.982428	13.560039	-0.077966	4.818281
395.235006	7999.936084	13.565043	-0.078094	4.818265
394.912566	7999.941170	13.570048	-0.078034	4.818268
395.217815	7999.937946	13.575053	-0.078091	4.818265
395.165258	7999.961403	13.580058	-0.078081	4.818273
394.896083	7999.935682	13.585063	-0.078031	4.818266
395.100724	7999.934248	13.590067	-0.078069	4.818265
395.349521	7999.921852	13.595072	-0.078115	4.818260
394.961833	7999.946022	13.600077	-0.078043	4.818269
395.113103	7999.938610	13.605082	-0.078071	4.818266
395.042575	7999.961823	13.610087	-0.078058	4.818273
394.612018	7999.988565	13.615091	-0.077978	4.818283
394.979356	7999.910514	13.620096	-0.078046	4.818258
395.059446	7999.917902	13.625101	-0.078061	4.818260
395.020270	7999.965712	13.630106	-0.078054	4.818275
394.813933	7999.920874	13.635111	-0.078015	4.818262
395.081963	7999.922401	13.640115	-0.078065	4.818261
394.799593	7999.916470	13.645120	-0.078013	4.818261
394.996101	7999.896008	13.650125	-0.078049	4.818254
394.498982	8000.010129	13.655130	-0.077957	4.818290
394.656674	7999.949205	13.660135	-0.077986	4.818271
394.747387	7999.937820	13.665139	-0.078003	4.818267
394.631554	7999.970928	13.670144	-0.077981	4.818278
394.638429	7999.967865	13.675149	-0.077982	4.818277
394.984206	7999.972548	13.680154	-0.078047	4.818277
394.880670	7999.935409	13.685159	-0.078027	4.818266
395.049085	7999.947146	13.690163	-0.078059	4.818269
395.193738	7999.951205	13.695168	-0.078086	4.818270
395.067809	7999.927425	13.700173	-0.078062	4.818263
395.392650	7999.940232	13.705178	-0.078122	4.818265
394.442990	7999.969399	13.710183	-0.077946	4.818278
394.759194	7999.972629	13.715187	-0.078004	4.818278
394.549735	7999.996062	13.720192	-0.077965	4.818285
394.654289	7999.997475	13.725197	-0.077985	4.818285
394.829245	7999.996690	13.730202	-0.078017	4.818285
394.674170	7999.984076	13.735207	-0.077988	4.818281
394.889689	7999.973330	13.740211	-0.078029	4.818277
395.300242	7999.951566	13.745216	-0.078105	4.818269
394.985566	7999.924177	13.750221	-0.078046	4.818262
394.909193	7999.955719	13.755226	-0.078032	4.818272
394.591519	7999.991347	13.760231	-0.077973	4.818284
394.882067	7999.981619	13.765235	-0.078027	4.818280
394.980348	7999.986100	13.770240	-0.078045	4.818281
394.891740	7999.988049	13.775245	-0.078029	4.818282
395.126057	8000.025903	13.780250	-0.078072	4.818292
394.874440	7999.983604	13.785255	-0.078025	4.818280
395.351435	7999.953282	13.790259	-0.078114	4.818270
395.087745	7999.977030	13.795264	-0.078065	4.818278
394.911089	7999.932594	13.800269	-0.078032	4.818265
394.753793	8000.015587	13.805274	-0.078003	4.818290
394.475822	8000.054907	13.810279	-0.077951	4.818303
395.039073	7999.961644	13.815283	-0.078056	4.818273
394.868849	7999.950926	13.820288	-0.078024	4.818271
394.555014	7999.982403	13.825293	-0.077965	4.818281
394.966474	7999.993230	13.830298	-0.078042	4.818283
395.353307	7999.907036	13.835303	-0.078114	4.818256
394.910021	7999.977745	13.840307	-0.078031	4.818279
394.864937	8000.051750	13.845312	-0.078023	4.818301
394.316292	8000.096859	13.850317	-0.077921	4.818316
394.705416	8000.096875	13.855322	-0.077993	4.818315
395.047837	8000.004823	13.860327	-0.078057	4.818286
395.010298	8000.004311	13.865331	-0.078050	4.818286
395.119957	7999.961654	13.870336	-0.078070	4.818273
394.402562	8000.083299	13.875341	-0.077937	4.818312
394.918653	8000.028283	13.880346	-0.078033	4.818294
394.697002	7999.994798	13.885351	-0.077991	4.818285
394.452892	8000.075564	13.890355	-0.077946	4.818310
394.792221	8000.021305	13.895360	-0.078009	4.818292
394.814984	7999.977470	13.900365	-0.078013	4.818279
394.813066	8000.061518	13.905370	-0.078013	4.818304
394.905555	7999.954519	13.910375	-0.078030	4.818272
395.058088	7999.982857	13.915379	-0.078058	4.818280
394.884829	7999.978404	13.920384	-0.078026	4.818279
395.429664	7999.906962	13.925389	-0.078127	4.818256
394.984054	8000.050157	13.930394	-0.078044	4.818300
394.791585	7999.980284	13.935399	-0.078009	4.818280
394.997981	7999.978873	13.940403	-0.078047	4.818279
395.369119	7999.975492	13.945408	-0.078116	4.818276
394.993631	7999.987216	13.950413	-0.078046	4.818281
395.219563	7999.935624	13.955418	-0.078088	4.818265
394.816633	8000.025798	13.960423	-0.078013	4.818293
395.096391	7999.947611	13.965427	-0.078065	4.818269
395.156150	7999.925297	13.970432	-0.078076	4.818262
394.863596	7999.909769	13.975437	-0.078022	4.818259
395.303948	7999.936752	13.980442	-0.078104	4.818265
395.553691	7999.893891	13.985447	-0.078150	4.818251
395.054373	7999.910242	13.990451	-0.078057	4.818258
394.929081	7999.981057	13.995456	-0.078034	4.818280
394.701171	7999.976915	14.000461	-0.077991	4.818279
395.259939	7999.959261	14.005466	-0.078095	4.818272
395.568962	7999.925611	14.010471	-0.078153	4.818261
394.921212	8000.014569	14.015475	-0.078032	4.818290
394.758844	8000.019722	14.020480	-0.078002	4.818292
394.574509	7999.990947	14.025485	-0.077967	4.818284
394.952828	8000.024446	14.030490	-0.078038	4.818292
394.867378	7999.969686	14.035495	-0.078022	4.818276
394.612467	7999.970432	14.040499	-0.077974	4.818278
395.044669	7999.953165	14.045504	-0.078055	4.818271
395.204463	7999.928002	14.050509	-0.078084	4.818263
395.252712	7999.930755	14.055514	-0.078093	4.818263
394.456855	8000.021910	14.060519	-0.077945	4.818294
394.867236	7999.951798	14.065523	-0.078021	4.818271
394.594344	8000.037429	14.070528	-0.077971	4.818298
394.512466	7999.957495	14.075533	-0.077955	4.818274
395.286166	7999.932243	14.080538	-0.078099	4.818264
394.530471	8000.053369	14.085543	-0.077959	4.818303
394.338523	8000.059172	14.090547	-0.077923	4.818305
394.225678	8000.129105	14.095552	-0.077902	4.818326
394.455599	8000.053396	14.100557	-0.077945	4.818303
394.677349	8000.029072	14.105562	-0.077986	4.818295
394.776509	7999.969457	14.110567	-0.078004	4.818277
394.879199	8000.024445	14.115571	-0.078023	4.818293
394.446942	8000.110017	14.120576	-0.077943	4.818320
394.303878	8000.063935	14.125581	-0.077916	4.818307
394.925504	7999.991432	14.130586	-0.078032	4.818283
395.210465	7999.916468	14.135591	-0.078085	4.818259
395.396947	7999.901126	14.140595	-0.078119	4.818254
395.148038	7999.960807	14.145600	-0.078073	4.818273
394.822632	7999.990025	14.150605	-0.078012	4.818283
394.799636	8000.055921	14.155610	-0.078008	4.818302
394.843390	8000.010268	14.160615	-0.078016	4.818289
395.069324	7999.973390	14.165619	-0.078058	4.818277
394.919784	7999.966106	14.170624	-0.078030	4.818275
395.037797	7999.931969	14.175629	-0.078052	4.818265
395.624335	7999.929405	14.180634	-0.078161	4.818261
395.108669	7999.930821	14.185639	-0.078065	4.818264
395.193811	7999.954042	14.190643	-0.078081	4.818270
395.376134	7999.907114	14.195648	-0.078115	4.818256
395.403765	7999.909587	14.200653	-0.078120	4.818256
395.222469	7999.948115	14.205658	-0.078086	4.818269
395.512865	7999.892142	14.210663	-0.078140	4.818251
395.660954	7999.880484	14.215667	-0.078168	4.818247
395.758635	7999.921741	14.220672	-0.078186	4.818259
395.536004	7999.898752	14.225677	-0.078145	4.818253
395.720247	7999.931724	14.230682	-0.078179	4.818262
395.638455	7999.894879	14.235687	-0.078164	4.818251
395.260967	7999.953869	14.240691	-0.078093	4.818270
395.076046	7999.957665	14.245696	-0.078059	4.818272
394.849985	8000.016605	14.250701	-0.078017	4.818290
395.145917	7999.973319	14.255706	-0.078072	4.818276
394.848048	7999.949311	14.260711	-0.078016	4.818270
395.267438	7999.962348	14.265715	-0.078094	4.818273
395.753240	7999.931095	14.270720	-0.078185	4.818261
395.331800	7999.920125	14.275725	-0.078106	4.818260
395.525610	7999.914340	14.280730	-0.078142	4.818257
395.372124	7999.881779	14.285735	-0.078114	4.818248
395.454353	7999.936490	14.290739	-0.078129	4.818264
395.663721	7999.924611	14.295744	-0.078168	4.818260
395.333312	7999.915925	14.300749	-0.078106	4.818259
395.331667	7999.929562	14.305754	-0.078106	4.818263
395.272004	7999.902476	14.310759	-0.078095	4.818255
395.870018	7999.914783	14.315763	-0.078206	4.818256
395.548771	7999.900966	14.320768	-0.078146	4.818253
395.844864	7999.871345	14.325773	-0.078201	4.818243
395.899401	7999.649276	14.330778	-0.078211	4.818177

395.651767	7996.470241	14.335783	-0.078163	4.817234
395.180016	7990.863374	14.340787	-0.078071	4.815569
395.717643	7984.138963	14.345792	-0.078167	4.813568
395.378468	7976.799176	14.350797	-0.078099	4.811386
395.842581	7969.094455	14.355802	-0.078180	4.809092
395.436169	7961.399037	14.360807	-0.078100	4.806803
395.633415	7953.420473	14.365811	-0.078131	4.804426
395.208003	7945.637185	14.370816	-0.078047	4.802108
395.327660	7937.535657	14.375821	-0.078064	4.799692
395.483114	7929.580903	14.380826	-0.078088	4.797319
395.647436	7921.525552	14.385831	-0.078113	4.794914
396.001538	7913.515041	14.390835	-0.078173	4.792521
395.788169	7905.531264	14.395840	-0.078129	4.790137
395.711545	7897.528005	14.400845	-0.078109	4.787745
395.427099	7889.574534	14.405850	-0.078051	4.785368
395.202061	7881.616379	14.410855	-0.078004	4.782987
394.769737	7873.644465	14.415859	-0.077918	4.780603
394.928409	7865.608793	14.420864	-0.077942	4.778196
394.636556	7857.555900	14.425869	-0.077883	4.775783
394.340837	7849.619600	14.430874	-0.077822	4.773405
394.330541	7841.550709	14.435879	-0.077815	4.770985
393.916786	7833.550730	14.440883	-0.077733	4.768585
393.805755	7825.534897	14.445888	-0.077707	4.766179
393.889457	7817.474030	14.450893	-0.077717	4.763757
394.192886	7809.562513	14.455898	-0.077768	4.761379
394.451554	7801.467616	14.460903	-0.077811	4.758944
394.313193	7793.520695	14.465907	-0.077780	4.756553
394.724672	7785.479769	14.470912	-0.077852	4.754132
394.602741	7777.501658	14.475917	-0.077824	4.751729
394.585624	7769.488072	14.480922	-0.077815	4.749315
394.631812	7761.486318	14.485927	-0.077819	4.746902
394.207812	7753.464361	14.490931	-0.077734	4.744484
393.649971	7745.604958	14.495936	-0.077625	4.742113
394.292984	7737.453385	14.500941	-0.077740	4.739651
394.536017	7729.499323	14.505946	-0.077780	4.737247
394.589680	7721.458079	14.510951	-0.077784	4.734817
394.777300	7713.460028	14.515955	-0.077814	4.732398
394.476659	7705.492788	14.520960	-0.077753	4.729988
394.114898	7697.488107	14.525965	-0.077680	4.727566
393.762545	7689.519682	14.530970	-0.077609	4.725153
393.794629	7681.513421	14.535975	-0.077610	4.722727
393.866347	7673.485757	14.540979	-0.077618	4.720293
393.695274	7665.536008	14.545984	-0.077581	4.717882
393.610245	7657.494175	14.550989	-0.077560	4.715441
393.614593	7649.522784	14.555994	-0.077556	4.713021
393.438121	7641.536124	14.560999	-0.077517	4.710595
393.445947	7633.491878	14.566003	-0.077514	4.708150
393.715908	7625.464279	14.571008	-0.077559	4.705708
393.748904	7617.406912	14.576013	-0.077559	4.703256
393.688980	7609.505099	14.581018	-0.077543	4.700851
393.644506	7601.485480	14.586023	-0.077530	4.698408
393.581794	7593.489450	14.591027	-0.077513	4.695971
393.863662	7585.473220	14.596032	-0.077560	4.693527
393.692483	7577.508675	14.601037	-0.077523	4.691097
393.407042	7569.510138	14.606042	-0.077464	4.688656
393.534901	7561.490522	14.611047	-0.077483	4.686207
393.614550	7553.412614	14.616051	-0.077492	4.683739
393.356024	7545.575970	14.621056	-0.077439	4.681343
393.126197	7537.496566	14.626061	-0.077391	4.678872
392.879934	7529.591815	14.631066	-0.077340	4.676453
392.772048	7521.500908	14.636071	-0.077315	4.673976
392.794914	7513.441060	14.641075	-0.077313	4.671507
392.844858	7505.429301	14.646080	-0.077318	4.669051
392.681105	7497.431631	14.651085	-0.077282	4.666598
393.117136	7489.344343	14.656090	-0.077358	4.664117
392.847275	7481.512639	14.661095	-0.077302	4.661712
392.923605	7473.432343	14.666099	-0.077311	4.659230
392.804243	7465.491289	14.671104	-0.077284	4.656790
392.382860	7457.470082	14.676109	-0.077200	4.654324
392.532475	7449.507185	14.681114	-0.077223	4.651874
392.162990	7441.440947	14.686119	-0.077149	4.649391
391.927119	7433.486568	14.691123	-0.077099	4.646941
392.089823	7425.406685	14.696128	-0.077124	4.644451
391.931068	7417.478052	14.701133	-0.077090	4.642007
392.362678	7409.433822	14.706138	-0.077165	4.639525
392.326563	7401.458905	14.711143	-0.077153	4.637064
391.780163	7393.444362	14.716147	-0.077046	4.634589
391.753861	7385.517465	14.721152	-0.077036	4.632139
391.717922	7377.379742	14.726157	-0.077024	4.629624
391.200135	7369.491501	14.731162	-0.076922	4.627184
391.746969	7361.356462	14.736167	-0.077018	4.624666
391.279735	7353.448556	14.741171	-0.076926	4.622217
391.779047	7345.387639	14.746176	-0.077014	4.619720
391.824815	7337.386409	14.751181	-0.077017	4.617240
391.403432	7329.424949	14.756186	-0.076933	4.614771
391.992806	7321.366420	14.761191	-0.077038	4.612271
391.654914	7313.368189	14.766195	-0.076970	4.609787
391.655133	7305.431572	14.771200	-0.076965	4.607322
391.962926	7297.343493	14.776205	-0.077017	4.604808
391.737638	7289.486498	14.781210	-0.076969	4.602365
391.420251	7281.423472	14.786215	-0.076905	4.599855
391.401603	7273.458005	14.791219	-0.076896	4.597376
391.240575	7265.460383	14.796224	-0.076861	4.594884
391.287174	7257.386128	14.801229	-0.076864	4.592368
390.826159	7249.370696	14.806234	-0.076773	4.589868
391.072387	7241.379404	14.811239	-0.076814	4.587375
390.981137	7233.311082	14.816243	-0.076792	4.584856
391.502366	7225.372943	14.821248	-0.076883	4.582378
391.175975	7217.322652	14.826253	-0.076817	4.579861
390.863832	7209.430562	14.831258	-0.076754	4.577393
390.787048	7201.360919	14.836263	-0.076735	4.574868
390.742905	7193.366366	14.841267	-0.076721	4.572366
390.994764	7185.323557	14.846272	-0.076763	4.569847
390.838206	7177.343479	14.851277	-0.076728	4.567346
390.510226	7169.372952	14.856282	-0.076662	4.564846
390.026012	7161.435844	14.861287	-0.076567	4.562355
389.876014	7153.370680	14.866291	-0.076533	4.559823
390.067098	7145.386125	14.871296	-0.076564	4.557316
390.145474	7137.312372	14.876301	-0.076573	4.554779
390.196419	7129.366393	14.881306	-0.076577	4.552281
390.232421	7121.348487	14.886311	-0.076579	4.549759
390.472391	7113.273906	14.891315	-0.076618	4.547218
390.291725	7105.347902	14.896320	-0.076579	4.544721
390.159156	7097.355607	14.901325	-0.076549	4.542202
390.457277	7089.298799	14.906330	-0.076599	4.539663
390.465226	7081.338954	14.911335	-0.076596	4.537152
390.156135	7073.330972	14.916339	-0.076533	4.534623
389.948839	7065.371132	14.921344	-0.076489	4.532109
390.277736	7057.234010	14.926349	-0.076545	4.529538
389.621478	7049.416761	14.931354	-0.076418	4.527065
389.694555	7041.285213	14.936359	-0.076426	4.524493
389.610456	7033.381682	14.941363	-0.076405	4.521991
389.862865	7025.331350	14.946368	-0.076447	4.519442
389.686798	7017.363741	14.951373	-0.076409	4.516916
389.522554	7009.326714	14.956378	-0.076373	4.514368
389.300937	7001.356890	14.961383	-0.076326	4.511838
389.823596	6993.212463	14.966387	-0.076418	4.509255
389.279747	6985.352570	14.971392	-0.076312	4.506757
389.313430	6977.196117	14.976397	-0.076313	4.504165
389.781826	6969.285760	14.981402	-0.076395	4.501651
389.551866	6961.214123	14.986407	-0.076347	4.499083
389.165098	6953.265727	14.991411	-0.076269	4.496551
389.386249	6945.208829	14.996416	-0.076305	4.493986
389.287755	6937.233809	15.001421	-0.076282	4.491444
388.695360	6929.306675	15.006426	-0.076166	4.488914
389.374014	6921.234212	15.011431	-0.076287	4.486341
388.942609	6913.254630	15.016435	-0.076202	4.483792
389.106842	6905.291569	15.021440	-0.076227	4.481249
388.763926	6897.246885	15.026445	-0.076158	4.478676
388.827637	6889.313766	15.031450	-0.076165	4.476140
388.434384	6881.309392	15.036455	-0.076086	4.473577
388.651221	6873.235078	15.041459	-0.076121	4.470993
388.831984	6865.235035	15.046464	-0.076150	4.468431
388.868186	6857.189954	15.051469	-0.076151	4.465852
388.656283	6849.228982	15.056474	-0.076106	4.463298
389.116102	6841.223986	15.061479	-0.076187	4.460732
388.758014	6833.262693	15.066483	-0.076115	4.458174
388.395709	6825.263436	15.071488	-0.076042	4.455602
388.538332	6817.232184	15.076493	-0.076063	4.453021
388.640438	6809.205190	15.081498	-0.076077	4.450440
388.235974	6801.244989	15.086503	-0.075997	4.447876
388.325778	6793.184858	15.091507	-0.076008	4.445281
388.060344	6785.308450	15.096512	-0.075953	4.442742
387.817050	6777.236867	15.101517	-0.075903	4.440138
387.657255	6769.298415	15.106522	-0.075868	4.437577
387.504133	6761.264909	15.111527	-0.075834	4.434983
387.496257	6753.230850	15.116531	-0.075827	4.432388
387.069746	6745.267487	15.121536	-0.075743	4.429813
387.539453	6737.146915	15.126541	-0.075825	4.427190
387.577865	6729.159010	15.131546	-0.075827	4.424606
387.283490	6721.287629	15.136551	-0.075767	4.422056
387.216330	6713.170227	15.141555	-0.075749	4.419426
387.488765	6705.206674	15.146560	-0.075794	4.416847
387.468682	6697.142269	15.151565	-0.075785	4.414231
387.740822	6689.158129	15.156570	-0.075831	4.411642
387.556818	6681.167754	15.161575	-0.075791	4.409047
387.668428	6673.149760	15.166579	-0.075807	4.406443
387.816290	6665.171315	15.171584	-0.075829	4.403851
387.108717	6657.239684	15.176589	-0.075692	4.401266
387.120627	6649.248358	15.181594	-0.075689	4.398666
386.788911	6641.304848	15.186599	-0.075622	4.396077
386.501171	6633.244602	15.191603	-0.075563	4.393449
387.004378	6625.231094	15.196608	-0.075652	4.390840
386.938607	6617.225868	15.201613	-0.075634	4.388228
387.086308	6609.180979	15.206618	-0.075656	4.385603
387.340668	6601.164484	15.211623	-0.075698	4.382986
386.976323	6593.254220	15.216627	-0.075625	4.380399
386.986773	6585.276102	15.221632	-0.075622	4.377790
386.607797	6577.234588	15.226637	-0.075546	4.375156
386.570142	6569.317653	15.231642	-0.075534	4.372564
386.560888	6561.258106	15.236647	-0.075527	4.369924
386.866935	6553.234742	15.241651	-0.075579	4.367296
386.996028	6545.214226	15.246656	-0.075597	4.364666
386.634884	6537.302443	15.251661	-0.075525	4.362067
386.550692	6529.253491	15.256666	-0.075504	4.359423
386.523494	6521.268034	15.261671	-0.075494	4.356799
386.811829	6513.177786	15.266675	-0.075542	4.354142
386.965288	6505.164686	15.271680	-0.075565	4.351507
386.751010	6497.156267	15.276685	-0.075520	4.348869
387.048345	6489.181741	15.281690	-0.075570	4.346245
386.479335	6481.250072	15.286695	-0.075459	4.343626
386.312908	6473.275173	15.291699	-0.075423	4.340995
386.672449	6465.222749	15.296704	-0.075485	4.338341
386.702362	6457.245366	15.301709	-0.075485	4.335707
386.657089	6449.259519	15.306714	-0.075471	4.333068
386.258180	6441.284302	15.311719	-0.075392	4.330429
386.074632	6433.283379	15.316723	-0.075352	4.327780
386.464145	6425.215803	15.321728	-0.075420	4.325113
386.231556	6417.289118	15.326733	-0.075371	4.322486
386.274377	6409.254043	15.331738	-0.075374	4.319824
386.436147	6401.268915	15.336743	-0.075399	4.317177
386.228908	6393.180422	15.341747	-0.075355	4.314492
386.444049	6385.268613	15.346752	-0.075390	4.311867
386.131550	6377.223896	15.351757	-0.075326	4.309191
385.842418	6369.291673	15.356762	-0.075267	4.306552
385.586061	6361.269750	15.361767	-0.075214	4.303881
385.588192	6353.265793	15.366771	-0.075209	4.301217
385.622820	6345.213459	15.371776	-0.075210	4.298536
385.694836	6337.182938	15.376781	-0.075218	4.295860
385.947719	6329.161883	15.381786	-0.075260	4.293188
386.020912	6321.199246	15.386791	-0.075269	4.290532
385.655623	6313.199288	15.391795	-0.075195	4.287858
385.595756	6305.213818	15.396800	-0.075179	4.285189
385.913354	6297.176206	15.401805	-0.075233	4.282505
385.758170	6289.237887	15.406810	-0.075199	4.279848
385.499163	6281.284176	15.411815	-0.075145	4.277184
384.970560	6273.275141	15.416819	-0.075042	4.274496
384.885612	6265.299694	15.421824	-0.075020	4.271823
384.884632	6257.204024	15.426829	-0.075015	4.269108
384.950392	6249.186920	15.431834	-0.075022	4.266418
385.155258	6241.141992	15.436839	-0.075055	4.263719
385.169328	6233.169907	15.441843	-0.075052	4.261040
385.404882	6225.204664	15.446848	-0.075091	4.258365
384.788237	6217.207464	15.451853	-0.074971	4.255668
384.446541	6209.240758	15.456858	-0.074902	4.252983
384.105262	6201.259760	15.461863	-0.074833	4.250291
384.808295	6193.153294	15.466867	-0.074959	4.247566
384.495058	6185.162275	15.471872	-0.074895	4.244868
384.443906	6177.201734	15.476877	-0.074880	4.242181
384.397427	6169.171263	15.481882	-0.074866	4.239468
384.731646	6161.212651	15.486887	-0.074923	4.236782
384.600342	6153.150731	15.491891	-0.074894	4.234055
384.892263	6145.188695	15.496896	-0.074943	4.231364
384.098417	6137.205091	15.501901	-0.074790	4.228653
383.917727	6129.211124	15.506906	-0.074751	4.225943
384.398542	6121.143201	15.511911	-0.074835	4.223213
383.721988	6113.204047	15.516915	-0.074704	4.220512
383.850735	6105.245097	15.521920	-0.074723	4.217812
383.684239	6097.177692	15.526925	-0.074686	4.215070
383.628596	6089.212987	15.531930	-0.074671	4.212362
384.046779	6081.127694	15.536935	-0.074743	4.209617
384.379573	6073.127377	15.541939	-0.074800	4.206898
384.020089	6065.168024	15.546944	-0.074728	4.204183
384.158904	6057.184428	15.551949	-0.074748	4.201465
384.111397	6049.193016	15.556954	-0.074734	4.198739
383.653762	6041.282022	15.561959	-0.074644	4.196034
384.100181	6033.153511	15.566963	-0.074722	4.193264
383.718139	6025.164595	15.571968	-0.074645	4.190530
383.453846	6017.156909	15.576973	-0.074591	4.187790
383.035403	6009.193688	15.581978	-0.074508	4.185060
383.382264	6001.193627	15.586983	-0.074567	4.182326
383.225091	5993.149847	15.591987	-0.074532	4.179568
383.215339	5985.210039	15.596992	-0.074525	4.176847
382.957246	5977.175046	15.601997	-0.074472	4.174087
382.946542	5969.230306	15.607002	-0.074465	4.171360
382.803649	5961.208284	15.612007	-0.074433	4.168603
382.546092	5953.184875	15.617011	-0.074380	4.165842
382.464244	5945.229494	15.622016	-0.074359	4.163105
382.386846	5937.230253	15.627021	-0.074340	4.160351
382.477902	5929.216579	15.632026	-0.074351	4.157593
383.125865	5921.117938	15.637031	-0.074467	4.154810
382.705425	5913.178980	15.642035	-0.074383	4.152067
382.837976	5905.143457	15.647040	-0.074403	4.149296
382.698391	5897.179479	15.652045	-0.074371	4.146544
382.829299	5889.164612	15.657050	-0.074390	4.143777
382.436127	5881.264232	15.662055	-0.074312	4.141040
382.342582	5873.215333	15.667059	-0.074289	4.138254
382.305791	5865.231030	15.672064	-0.074277	4.135489
382.003076	5857.235276	15.677069	-0.074216	4.132715
382.104481	5849.176316	15.682074	-0.074229	4.129922
382.190736	5841.194428	15.687079	-0.074240	4.127154
382.301957	5833.108115	15.692083	-0.074255	4.124349
382.175130	5825.286343	15.697088	-0.074227	4.121630
382.094407	5817.219289	15.702093	-0.074206	4.118824
382.109099	5809.241920	15.707098	-0.074204	4.116049
382.769116	5801.157312	15.712103	-0.074321	4.113244
382.461836	5793.163182	15.717107	-0.074259	4.110455
382.812123	5785.172393	15.722112	-0.074319	4.107675
382.211937	5777.218054	15.727117	-0.074202	4.104892
381.861834	5769.295890	15.732122	-0.074131	4.102122
381.570124	5761.291968	15.737127	-0.074072	4.099322
381.812647	5753.206601	15.742131	-0.074112	4.096499
381.694047	5745.197775	15.747136	-0.074084	4.093696
381.145790	5737.242554	15.752141	-0.073977	4.090904
381.056147	5729.231198	15.757146	-0.073955	4.088097
381.083803	5721.224950	15.762151	-0.073955	4.085291
381.296103	5713.181761	15.767155	-0.073989	4.082473
381.328485	5705.180071	15.772160	-0.073990	4.079665
381.741112	5697.177584	15.777165	-0.074062	4.076861
380.932262	5689.236752	15.782170	-0.073906	4.074058
380.970373	5681.267371	15.787175	-0.073908	4.071255
381.096715	5673.164901	15.792179	-0.073926	4.068406
381.366949	5665.148709	15.797184	-0.073971	4.065587
381.081572	5657.229299	15.802189	-0.073913	4.062791
381.224841	5649.148181	15.807194	-0.073934	4.059943
381.506648	5641.193974	15.812199	-0.073981	4.057140
381.301145	5633.156050	15.817203	-0.073938	4.054298
381.402040	5625.257839	15.822208	-0.073951	4.051508
381.625430	5617.145183	15.827213	-0.073987	4.048643
381.593247	5609.184452	15.832218	-0.073976	4.045825
381.397712	5601.240098	15.837223	-0.073935	4.043008
381.213653	5593.235691	15.842227	-0.073895	4.040168
381.110672	5585.330146	15.847232	-0.073871	4.037363
381.501650	5577.202940	15.852237	-0.073938	4.034485
381.261161	5569.220748	15.857242	-0.073888	4.031646
380.972104	5561.229815	15.862247	-0.073829	4.028801
380.897518	5553.183069	15.867251	-0.073810	4.025938
380.589746	5545.277315	15.872256	-0.073747	4.023119
380.664957	5537.239521	15.877261	-0.073756	4.020258
380.740742	5529.277447	15.882266	-0.073765	4.017421
380.790455	5521.197062	15.887271	-0.073769	4.014540
380.644090	5513.254037	15.892275	-0.073736	4.011702
380.128801	5505.295568	15.897280	-0.073635	4.008851
380.410713	5497.206762	15.902285	-0.073682	4.005964
381.278745	5489.107286	15.907290	-0.073839	4.003082
381.095800	5481.241072	15.912295	-0.073800	4.000263
380.325073	5473.321396	15.917299	-0.073651	3.997413
380.081042	5465.318052	15.922304	-0.073600	3.994539
380.590545	5457.234753	15.927309	-0.073690	3.991648
380.572846	5449.207766	15.932314	-0.073681	3.988767
380.427361	5441.275318	15.937319	-0.073649	3.985914
380.103968	5433.296508	15.942323	-0.073583	3.983040
380.059976	5425.341177	15.947328	-0.073570	3.980177
380.092957	5417.288135	15.952333	-0.073571	3.977278
380.216345	5409.228708	15.957338	-0.073588	3.974377
380.358845	5401.262465	15.962343	-0.073610	3.971507
380.087476	5393.240300	15.967347	-0.073554	3.968608
380.041826	5385.294981	15.972352	-0.073540	3.965738
380.149716	5377.276938	15.977357	-0.073555	3.962843
380.194223	5369.254090	15.982362	-0.073558	3.959942
380.074377	5361.309212	15.987367	-0.073531	3.957065
380.168763	5353.227476	15.992371	-0.073543	3.954140
380.178317	5345.273112	15.997376	-0.073539	3.951258
379.738265	5337.308759	16.002381	-0.073452	3.948361
379.084028	5329.363127	16.007386	-0.073325	3.945465
379.541011	5321.270285	16.012391	-0.073405	3.942534
379.036796	5313.306687	16.017395	-0.073306	3.939630
379.616398	5305.270767	16.022400	-0.073408	3.936718
379.341468	5297.308105	16.027405	-0.073352	3.933814
378.925527	5289.318537	16.032410	-0.073269	3.930895
378.860552	5281.332979	16.037415	-0.073252	3.927983
378.873210	5273.240662	16.042419	-0.073249	3.925031
379.412050	5265.263447	16.047424	-0.073344	3.922129
378.936613	5257.319124	16.052429	-0.073250	3.919217
379.030785	5249.313100	16.057434	-0.073263	3.916291
378.954342	5241.325533	16.062439	-0.073243	3.913367
379.095181	5233.272695	16.067443	-0.073264	3.910420
379.057966	5225.289936	16.072448	-0.073252	3.907494
379.046443	5217.257335	16.077453	-0.073244	3.904548
379.187629	5209.329685	16.082458	-0.073266	3.901641
378.632242	5201.398122	16.087463	-0.073157	3.898717
378.218668	5193.428523	16.092467	-0.073075	3.895779
378.766594	5185.310746	16.097472	-0.073171	3.892804
378.728706	5177.273475	16.102477	-0.073159	3.889844
378.695718	5169.303064	16.107482	-0.073148	3.886907
378.573479	5161.330933	16.112487	-0.073120	3.883965
377.902167	5153.488384	16.117491	-0.072989	3.881057
378.151418	5145.397104	16.122496	-0.073031	3.878075
378.224581	5137.368227	16.127501	-0.073039	3.875109
378.146877	5129.254354	16.132506	-0.073019	3.872107
378.348387	5121.247473	16.137511	-0.073051	3.869147
377.987354	5113.274165	16.142515	-0.072979	3.866186
378.255194	5105.290887	16.147520	-0.073024	3.863233
377.501947	5097.422086	16.152525	-0.072878	3.860298
377.143810	5089.467309	16.157530	-0.072806	3.857337
377.625355	5081.317905	16.162535	-0.072891	3.854319
377.790063	5073.361562	16.167539	-0.072916	3.851364
377.774434	5065.334426	16.172544	-0.072908	3.848377
377.437642	5057.351367	16.177549	-0.072840	3.845396
377.495207	5049.377745	16.182554	-0.072845	3.842426
377.515662	5041.363064	16.187559	-0.072844	3.839437
376.991744	5033.437390	16.192563	-0.072741	3.836467
377.787070	5025.302169	16.197568	-0.072884	3.833445
377.182709	5017.433046	16.202573	-0.072766	3.830490
377.137189	5009.360502	16.207578	-0.072752	3.827468
377.716184	5001.318268	16.212583	-0.072855	3.824470
377.721236	4993.377773	16.217587	-0.072851	3.821494
378.035280	4985.352682	16.222592	-0.072904	3.818491
377.259086	4977.430469	16.227597	-0.072754	3.815500
376.863245	4969.447164	16.232602	-0.072675	3.812493
377.195911	4961.385876	16.237607	-0.072732	3.809470
377.051173	4953.404426	16.242611	-0.072700	3.806463
377.330089	4945.378031	16.247616	-0.072746	3.803448
377.488088	4937.377648	16.252621	-0.072770	3.800436
377.161013	4929.462723	16.257626	-0.072704	3.797444
376.737530	4921.472426	16.262631	-0.072620	3.794418
376.822931	4913.450083	16.267635	-0.072631	3.791390
376.518457	4905.477891	16.272640	-0.072569	3.788369
376.326000	4897.454976	16.277645	-0.072528	3.785329
376.316656	4889.480844	16.282650	-0.072521	3.782310
376.795300	4881.411993	16.287655	-0.072605	3.779263
376.690542	4873.430186	16.292659	-0.072580	3.776234
376.813921	4865.425796	16.297664	-0.072598	3.773198
376.878743	4857.392032	16.302669	-0.072604	3.770148
376.824790	4849.438699	16.307674	-0.072589	3.767123
376.852128	4841.425966	16.312679	-0.072589	3.764075
376.832477	4833.484974	16.317683	-0.072580	3.761051
376.535639	4825.501625	16.322688	-0.072519	3.758001
376.228870	4817.541071	16.327693	-0.072457	3.754958
376.347778	4809.519085	16.332698	-0.072474	3.751899
376.313905	4801.494581	16.337703	-0.072462	3.748832
376.267057	4793.442401	16.342707	-0.072448	3.745752
376.266018	4785.512990	16.347712	-0.072443	3.742718
375.888500	4777.556464	16.352717	-0.072367	3.739662
376.049780	4769.531832	16.357722	-0.072392	3.736590
376.354542	4761.493840	16.362727	-0.072444	3.733514
376.290391	4753.482310	16.367731	-0.072426	3.730437
376.511751	4745.492885	16.372736	-0.072462	3.727372
376.030331	4737.521091	16.377741	-0.072368	3.724295
376.101024	4729.569284	16.382746	-0.072376	3.721236
375.830064	4721.610050	16.387751	-0.072320	3.718163
375.521868	4713.608174	16.392755	-0.072257	3.715071
375.465049	4705.575410	16.397760	-0.072241	3.711970
375.336346	4697.541239	16.402765	-0.072212	3.708864
375.004386	4689.524993	16.407770	-0.072145	3.705758
375.306142	4681.492602	16.412775	-0.072196	3.702658
375.768928	4673.433436	16.417779	-0.072277	3.699550
374.941093	4665.647274	16.422784	-0.072118	3.696512
375.220734	4657.548524	16.427789	-0.072164	3.693379
375.253180	4649.535970	16.432794	-0.072165	3.690270
375.070333	4641.581724	16.437799	-0.072126	3.687175
374.568855	4633.599734	16.442803	-0.072027	3.684059
374.968577	4625.624185	16.447808	-0.072096	3.680966
374.595832	4617.666358	16.452813	-0.072022	3.677857
374.626292	4609.614900	16.457818	-0.072022	3.674720
375.092824	4601.570701	16.462823	-0.072104	3.671595
374.977882	4593.579672	16.467827	-0.072077	3.668472
375.120667	4585.554509	16.472832	-0.072098	3.665340
374.680772	4577.649996	16.477837	-0.072011	3.662237
374.948479	4569.569998	16.482842	-0.072056	3.659081
374.488164	4561.706181	16.487847	-0.071965	3.655988
374.579869	4553.626747	16.492851	-0.071977	3.652822
374.792970	4545.609380	16.497856	-0.072011	3.649682
374.758237	4537.636126	16.502861	-0.071999	3.646549
374.107578	4529.701297	16.507866	-0.071873	3.643412
374.570594	4521.651180	16.512871	-0.071954	3.640258
374.481884	4513.665209	16.517875	-0.071932	3.637110
374.681564	4505.664888	16.522880	-0.071964	3.633963
374.596392	4497.671167	16.527885	-0.071943	3.630807
374.778477	4489.630546	16.532890	-0.071972	3.627638
374.686608	4481.663907	16.537895	-0.071949	3.624487
374.684929	4473.663039	16.542899	-0.071944	3.621322
374.435088	4465.717810	16.547904	-0.071892	3.618170
374.308597	4457.732899	16.552909	-0.071863	3.615003
373.718183	4449.771368	16.557914	-0.071748	3.611829
373.927686	4441.718864	16.562919	-0.071782	3.608639
373.928456	4433.714528	16.567923	-0.071777	3.605459
373.606263	4425.789521	16.572928	-0.071711	3.602298
373.209368	4417.800246	16.577933	-0.071632	3.599107
373.339858	4409.747376	16.582938	-0.071651	3.595904
373.328345	4401.794279	16.587943	-0.071644	3.592733
373.541876	4393.706464	16.592947	-0.071678	3.589512
373.721823	4385.715035	16.597952	-0.071707	3.586325
373.611086	4377.735038	16.602957	-0.071681	3.583132
373.498829	4369.717865	16.607962	-0.071654	3.579921
373.512859	4361.802161	16.612967	-0.071652	3.576752
373.187404	4353.791185	16.617971	-0.071586	3.573531
373.500084	4345.751385	16.622976	-0.071639	3.570315
373.204040	4337.803331	16.627981	-0.071579	3.567115
373.425092	4329.729608	16.632986	-0.071614	3.563877
373.548631	4321.814016	16.637991	-0.071632	3.560696
373.108785	4313.872960	16.642995	-0.071545	3.557486
373.205992	4305.823361	16.648000	-0.071558	3.554245
373.165141	4297.824075	16.653005	-0.071545	3.551017
372.756948	4289.829222	16.658010	-0.071464	3.547776
373.115595	4281.755354	16.663015	-0.071525	3.544525
372.453427	4273.897478	16.668019	-0.071397	3.541326
372.818943	4265.844596	16.673024	-0.071460	3.538077
372.686061	4257.866662	16.678029	-0.071430	3.534840
372.253431	4249.922362	16.683034	-0.071344	3.531605
372.527382	4241.862349	16.688039	-0.071390	3.528341
371.786192	4233.954622	16.693043	-0.071246	3.525105
371.755525	4225.972285	16.698048	-0.071235	3.521857
371.974133	4217.915767	16.703053	-0.071271	3.518584
372.161606	4209.847644	16.708058	-0.071300	3.515303
372.057502	4201.926162	16.713063	-0.071276	3.512069
371.692463	4193.937012	16.718067	-0.071203	3.508796
371.653332	4185.903050	16.723072	-0.071190	3.505512
371.991789	4177.878825	16.728077	-0.071248	3.502241
371.825520	4169.888999	16.733082	-0.071212	3.498965
371.889707	4161.947065	16.738087	-0.071218	3.495712
371.845815	4153.918392	16.743091	-0.071205	3.492418
371.829671	4145.911068	16.748096	-0.071197	3.489130
372.124700	4137.906898	16.753101	-0.071246	3.485851
371.951734	4129.959063	16.758106	-0.071209	3.482576
371.834983	4121.998349	16.763111	-0.071182	3.479295
371.426722	4114.045233	16.768115	-0.071101	3.476004
372.232800	4105.892000	16.773120	-0.071245	3.472668
371.835359	4098.013794	16.778125	-0.071166	3.469402
371.132995	4090.083386	16.783130	-0.071030	3.466101
371.213863	4082.091071	16.788135	-0.071040	3.462798
371.259593	4074.040637	16.793139	-0.071043	3.459466
371.201316	4066.042588	16.798144	-0.071027	3.456149
371.075443	4058.053278	16.803149	-0.070998	3.452830
370.938979	4050.058306	16.808154	-0.070968	3.449506
371.014161	4042.081453	16.813159	-0.070977	3.446193
371.145677	4034.027339	16.818163	-0.070996	3.442846
371.253657	4026.043639	16.823168	-0.071011	3.439525
371.205829	4018.099243	16.828173	-0.070996	3.436212
371.136932	4010.096236	16.833178	-0.070978	3.432870
371.025319	4002.134502	16.838183	-0.070952	3.429541
370.906312	3994.107284	16.843187	-0.070925	3.426180
371.137028	3986.094511	16.848192	-0.070963	3.422835
370.996079	3978.138536	16.853197	-0.070931	3.419497
370.711729	3970.195019	16.858202	-0.070873	3.416157
370.252174	3962.256339	16.863207	-0.070782	3.412808
370.371694	3954.141566	16.868211	-0.070799	3.409403
370.545403	3946.173458	16.873216	-0.070826	3.406058
370.387815	3938.196008	16.878221	-0.070792	3.402694
369.753621	3930.257450	16.883226	-0.070668	3.399326
369.891242	3922.300454	16.888231	-0.070689	3.395975
369.500081	3914.244947	16.893235	-0.070611	3.392559
369.304707	3906.217146	16.898240	-0.070569	3.389159
369.371772	3898.201517	16.903245	-0.070576	3.385770
369.366362	3890.203807	16.908250	-0.070570	3.382383
369.495227	3882.181190	16.913255	-0.070589	3.378986
369.702195	3874.164243	16.918259	-0.070622	3.375592
369.829949	3866.204736	16.923264	-0.070640	3.372215
370.290081	3858.125217	16.928269	-0.070721	3.368797
369.872438	3850.187983	16.933274	-0.070638	3.365403
369.661590	3842.307567	16.938279	-0.070593	3.362037
369.974584	3834.245231	16.943283	-0.070646	3.358610
370.185522	3826.262045	16.948288	-0.070680	3.355210
370.087738	3818.308846	16.953293	-0.070657	3.351807
369.867124	3810.306749	16.958298	-0.070611	3.348375
369.885651	3802.318838	16.963303	-0.070609	3.344955
369.572578	3794.400423	16.968307	-0.070545	3.341549
369.636824	3786.359383	16.973312	-0.070552	3.338101
369.683956	3778.372453	16.978317	-0.070556	3.334671
369.350828	3770.405776	16.983322	-0.070488	3.331233
369.073588	3762.436707	16.988327	-0.070431	3.327792
369.007100	3754.404329	16.993331	-0.070414	3.324328
369.094145	3746.451247	16.998336	-0.070425	3.320900
369.033760	3738.456698	17.003341	-0.070408	3.317446
369.082397	3730.384188	17.008346	-0.070412	3.313958
368.933815	3722.453306	17.013351	-0.070379	3.310521
368.930291	3714.440560	17.018355	-0.070373	3.307050
369.235887	3706.366520	17.023360	-0.070425	3.303561
368.890719	3698.493590	17.028365	-0.070355	3.300129
368.473591	3690.521382	17.033370	-0.070272	3.296649
368.813715	3682.455115	17.038375	-0.070330	3.293153
368.822525	3674.436807	17.043379	-0.070327	3.289662
368.502604	3666.543691	17.048384	-0.070262	3.286208
368.435972	3658.545003	17.053389	-0.070244	3.282715
368.161860	3650.588209	17.058394	-0.070188	3.279228
368.175854	3642.622771	17.063399	-0.070185	3.275745
367.846951	3634.624018	17.068403	-0.070119	3.272230
367.919278	3626.586968	17.073408	-0.070127	3.268711
368.173044	3618.553116	17.078413	-0.070169	3.265196
368.303986	3610.558377	17.083418	-0.070188	3.261690
368.496045	3602.549457	17.088423	-0.070219	3.258177
368.377827	3594.603527	17.093427	-0.070192	3.254675
368.251148	3586.650006	17.098432	-0.070163	3.251165
368.235641	3578.640266	17.103437	-0.070155	3.247631
368.093499	3570.605908	17.108442	-0.070123	3.244077
368.222165	3562.692616	17.113447	-0.070142	3.240584
368.181636	3554.698673	17.118451	-0.070129	3.237045
368.179581	3546.670425	17.123456	-0.070123	3.233488
368.016879	3538.716861	17.128461	-0.070088	3.229954
367.549662	3530.751747	17.133466	-0.069995	3.226397
367.861013	3522.695050	17.138471	-0.070048	3.222829
367.338028	3514.757359	17.143475	-0.069945	3.219275
367.476913	3506.753688	17.148480	-0.069966	3.215715
367.398484	3498.779574	17.153485	-0.069946	3.212155
367.564062	3490.716907	17.158490	-0.069972	3.208563
367.710856	3482.721538	17.163495	-0.069994	3.204995
367.670209	3474.761384	17.168499	-0.069981	3.201431
367.237188	3466.816560	17.173504	-0.069895	3.197854
367.495596	3458.803689	17.178509	-0.069938	3.194271
367.708161	3450.789522	17.183514	-0.069972	3.190682
367.396056	3442.856619	17.188519	-0.069909	3.187103
367.182726	3434.876742	17.193523	-0.069864	3.183502
367.152928	3426.878452	17.198528	-0.069853	3.179898
366.750110	3418.971956	17.203533	-0.069773	3.176314
366.796539	3410.901495	17.208538	-0.069776	3.172672
366.927357	3402.882409	17.213543	-0.069795	3.169052
366.382466	3394.975901	17.218547	-0.069689	3.165450
366.280519	3387.006919	17.223552	-0.069665	3.161835
366.079100	3379.052083	17.228557	-0.069622	3.158217
366.039535	3371.014925	17.233562	-0.069609	3.154565
365.932843	3363.001965	17.238567	-0.069584	3.150917
366.133269	3354.960393	17.243571	-0.069616	3.147266
365.930537	3347.028987	17.248576	-0.069573	3.143642
365.794145	3339.058520	17.253581	-0.069543	3.139999
366.183386	3330.956225	17.258586	-0.069610	3.136316
365.790335	3323.088688	17.263591	-0.069531	3.132700
365.406735	3315.080926	17.268595	-0.069455	3.129016
365.598211	3307.059218	17.273600	-0.069485	3.125348
365.779259	3299.067597	17.278605	-0.069513	3.121689
366.146911	3291.018279	17.283610	-0.069577	3.118007
366.118500	3283.079912	17.288615	-0.069566	3.114354
365.347994	3275.216979	17.293619	-0.069417	3.110697
365.673497	3267.136448	17.298624	-0.069473	3.106986
365.309298	3259.229243	17.303629	-0.069400	3.103319
365.556742	3251.145263	17.308634	-0.069441	3.099594
365.648521	3243.209424	17.313639	-0.069452	3.095926
365.282668	3235.243383	17.318643	-0.069379	3.092218
364.888147	3227.271852	17.323648	-0.069300	3.088501
365.227703	3219.210838	17.328653	-0.069358	3.084774
365.050754	3211.270713	17.333658	-0.069320	3.081073
365.056902	3203.286568	17.338663	-0.069316	3.077356
364.838558	3195.309726	17.343667	-0.069270	3.073628
365.285564	3187.200556	17.348672	-0.069348	3.069865
365.122988	3179.278236	17.353677	-0.069313	3.066155
365.020041	3171.280720	17.358682	-0.069288	3.062409
364.628456	3163.383582	17.363687	-0.069210	3.058691
364.675120	3155.358259	17.368691	-0.069213	3.054930
365.048661	3147.302811	17.373696	-0.069278	3.051165
365.051940	3139.307652	17.378701	-0.069273	3.047407
364.783867	3131.361962	17.383706	-0.069218	3.043654
364.156219	3123.529371	17.388711	-0.069096	3.039931
364.439920	3115.475631	17.393715	-0.069143	3.036145
364.562677	3107.446711	17.398720	-0.069161	3.032357
364.553154	3099.471356	17.403725	-0.069154	3.028584
364.158469	3091.501746	17.408730	-0.069075	3.024790
363.864916	3083.605350	17.413735	-0.069015	3.021030
364.082764	3075.534084	17.418739	-0.069051	3.017209
364.257776	3067.515533	17.423744	-0.069078	3.013405
363.927134	3059.586916	17.428749	-0.069011	3.009614
363.650361	3051.626731	17.433754	-0.068954	3.005806
363.733352	3043.611643	17.438759	-0.068965	3.001985
363.617399	3035.632525	17.443763	-0.068938	2.998166
363.458811	3027.663630	17.448768	-0.068903	2.994345
363.647670	3019.656046	17.453773	-0.068933	2.990518
363.368749	3011.680851	17.458778	-0.068876	2.986678
363.728043	3003.624055	17.463783	-0.068937	2.982827
363.539162	2995.679989	17.468787	-0.068897	2.978997
363.231478	2987.756468	17.473792	-0.068834	2.975165
363.405246	2979.726567	17.478797	-0.068862	2.971302
363.043865	2971.763032	17.483802	-0.068789	2.967438
363.261999	2963.744610	17.488807	-0.068824	2.963573
363.459019	2955.740764	17.493811	-0.068856	2.959709
363.058461	2947.869613	17.498816	-0.068776	2.955873
362.942837	2939.878820	17.503821	-0.068749	2.951988
362.619763	2931.898803	17.508826	-0.068684	2.948093
362.766815	2923.889590	17.513831	-0.068706	2.944203
362.772622	2915.920457	17.518835	-0.068702	2.940321
362.760546	2907.926085	17.523840	-0.068694	2.936419
363.134812	2899.858328	17.528845	-0.068759	2.932498
363.565093	2891.796902	17.533850	-0.068834	2.928577
362.945208	2883.969633	17.538855	-0.068713	2.924709
362.859468	2876.018277	17.543859	-0.068692	2.920804
363.075313	2868.002898	17.548864	-0.068727	2.916879
362.975932	2860.026839	17.553869	-0.068703	2.912951
362.659567	2852.023641	17.558874	-0.068639	2.908992
362.738839	2844.015908	17.563879	-0.068648	2.905047
362.888974	2836.009208	17.568883	-0.068671	2.901101
362.271863	2828.137560	17.573888	-0.068551	2.897174
362.265090	2820.155029	17.578893	-0.068544	2.893220
362.627541	2812.049517	17.583898	-0.068607	2.889221
362.245633	2804.179395	17.588903	-0.068530	2.885292
362.188620	2796.194542	17.593907	-0.068514	2.881318
362.075400	2788.242735	17.598912	-0.068488	2.877352
362.619952	2780.183248	17.603917	-0.068584	2.873364
362.247930	2772.235839	17.608922	-0.068510	2.869375
362.195196	2764.278480	17.613927	-0.068495	2.865393
361.936710	2756.355564	17.618931	-0.068441	2.861411
362.069855	2748.330224	17.623936	-0.068461	2.857395
361.866606	2740.374290	17.628941	-0.068418	2.853388
361.822093	2732.313501	17.633946	-0.068404	2.849333
361.579892	2724.431164	17.638951	-0.068354	2.845349
361.391923	2716.473357	17.643955	-0.068314	2.841326
361.826373	2708.396245	17.648960	-0.068389	2.837272
361.286463	2700.548463	17.653965	-0.068284	2.833272
361.312430	2692.463369	17.658970	-0.068283	2.829179
361.591735	2684.445656	17.663975	-0.068330	2.825130
361.025287	2676.582989	17.668979	-0.068219	2.821103
361.347123	2668.509531	17.673984	-0.068274	2.817016
361.311809	2660.552680	17.678989	-0.068262	2.812961
360.933098	2652.600066	17.683994	-0.068186	2.808882
360.873939	2644.629407	17.688999	-0.068170	2.804807
360.736353	2636.685590	17.694003	-0.068139	2.800735
360.347457	2628.738861	17.699008	-0.068061	2.796640
360.595099	2620.695592	17.704013	-0.068102	2.792528
360.853787	2612.647560	17.709018	-0.068145	2.788409
360.975485	2604.651579	17.714023	-0.068163	2.784301
361.263209	2596.661159	17.719027	-0.068211	2.780201
360.539427	2588.832109	17.724032	-0.068071	2.776116
360.493725	2580.841582	17.729037	-0.068057	2.771983
360.257653	2572.854715	17.734042	-0.068008	2.767835
360.162351	2564.910863	17.739047	-0.067985	2.763710
360.188366	2556.909285	17.744051	-0.067985	2.759557
359.922807	2548.978894	17.749056	-0.067930	2.755417
359.961954	2540.953110	17.754061	-0.067932	2.751240
360.094559	2532.864976	17.759066	-0.067951	2.747030
360.393700	2524.868465	17.764071	-0.068002	2.742871
360.059038	2516.988147	17.769075	-0.067934	2.738728
360.057311	2508.986085	17.774080	-0.067929	2.734535
360.121370	2501.013389	17.779085	-0.067935	2.730355
360.125910	2493.032101	17.784090	-0.067931	2.726161
359.868128	2485.140224	17.789095	-0.067878	2.721990
359.612216	2477.192902	17.794099	-0.067825	2.717784
359.743760	2469.131003	17.799104	-0.067844	2.713536
359.335613	2461.257667	17.804109	-0.067763	2.709346
358.865360	2453.306476	17.809114	-0.067670	2.705105
359.094333	2445.282802	17.814119	-0.067708	2.700863
358.630571	2437.393156	17.819123	-0.067616	2.696641
358.755789	2429.319755	17.824128	-0.067634	2.692353
358.742689	2421.348535	17.829133	-0.067626	2.688103
358.940831	2413.285893	17.834138	-0.067658	2.683811
359.293639	2405.323337	17.839143	-0.067718	2.679577
359.115426	2397.407763	17.844147	-0.067680	2.675326
358.909422	2389.445464	17.849152	-0.067636	2.671041
359.163696	2381.430927	17.854157	-0.067679	2.666752
358.804031	2373.501031	17.859162	-0.067606	2.662461
358.615221	2365.551543	17.864167	-0.067566	2.658163
358.533489	2357.578140	17.869171	-0.067546	2.653853
358.838431	2349.496199	17.874176	-0.067597	2.649503
358.661747	2341.607506	17.879181	-0.067559	2.645218
358.259843	2333.694591	17.884186	-0.067479	2.640898
358.445953	2325.708780	17.889191	-0.067508	2.636571
358.537469	2317.713322	17.894195	-0.067520	2.632225
358.248562	2309.747125	17.899200	-0.067461	2.627862
358.092831	2301.807729	17.904205	-0.067427	2.623515
358.105201	2293.805019	17.909210	-0.067424	2.619138
358.002602	2285.865330	17.914215	-0.067400	2.614780
358.010503	2277.859470	17.919219	-0.067396	2.610387
358.314741	2269.821444	17.924224	-0.067447	2.605988
358.205378	2261.912986	17.929229	-0.067422	2.601625
358.218325	2253.925019	17.934234	-0.067419	2.597219
358.054110	2245.969504	17.939239	-0.067383	2.592812
357.900613	2237.938351	17.944243	-0.067349	2.588355
357.349425	2230.034613	17.949248	-0.067241	2.583934
357.470708	2222.067280	17.954253	-0.067259	2.579517
357.292215	2214.119524	17.959258	-0.067220	2.575082
357.151947	2206.170921	17.964263	-0.067189	2.570642
356.870039	2198.218367	17.969267	-0.067131	2.566182
356.677795	2190.269514	17.974272	-0.067090	2.561722
356.623242	2182.307607	17.979277	-0.067075	2.557257
356.668624	2174.266855	17.984282	-0.067078	2.552747
356.793257	2166.293116	17.989287	-0.067096	2.548273
356.695261	2158.325798	17.994291	-0.067072	2.543778
356.726877	2150.340801	17.999296	-0.067073	2.539275
356.516630	2142.445690	18.004301	-0.067029	2.534797
356.704067	2134.425115	18.009306	-0.067058	2.530269
356.446025	2126.495105	18.014311	-0.067005	2.525751
356.613191	2118.510335	18.019315	-0.067031	2.521226
356.624518	2110.543480	18.024320	-0.067028	2.516691
356.655194	2102.572609	18.029325	-0.067028	2.512147
356.240229	2094.648747	18.034330	-0.066946	2.507589
356.553691	2086.617534	18.039335	-0.066999	2.503015
356.642256	2078.671898	18.044339	-0.067010	2.498465
356.000287	2070.791745	18.049344	-0.066885	2.493889
356.474590	2062.720305	18.054349	-0.066968	2.489279
356.479278	2054.749134	18.059354	-0.066964	2.484683
356.256733	2046.864782	18.064359	-0.066917	2.480111
355.978657	2038.940123	18.069363	-0.066860	2.475503
355.945938	2030.960306	18.074368	-0.066849	2.470874
356.061208	2022.981940	18.079373	-0.066865	2.466247
355.820480	2015.015425	18.084378	-0.066815	2.461592
356.178736	2007.008270	18.089383	-0.066877	2.456950
356.040028	1999.085803	18.094387	-0.066846	2.452311
356.249131	1991.057624	18.099392	-0.066879	2.447627
356.453747	1983.084085	18.104397	-0.066912	2.442967
355.904575	1975.255692	18.109402	-0.066805	2.438324
356.212749	1967.215751	18.114407	-0.066857	2.433615
355.510498	1959.335398	18.119411	-0.066721	2.428911
355.362550	1951.365635	18.124416	-0.066688	2.424189
355.067664	1943.453441	18.129421	-0.066628	2.419480
355.576038	1935.348503	18.134426	-0.066717	2.414712
355.875043	1927.353306	18.139431	-0.066768	2.409982
355.633797	1919.437490	18.144435	-0.066718	2.405247
355.229882	1911.567821	18.149440	-0.066637	2.400518
355.331868	1903.597284	18.154445	-0.066651	2.395760
355.577941	1895.560693	18.159450	-0.066692	2.390964
355.505359	1887.630195	18.164455	-0.066673	2.386196
355.837804	1879.609695	18.169459	-0.066729	2.381397
355.766681	1871.703816	18.174464	-0.066711	2.376626
355.322916	1863.842256	18.179469	-0.066623	2.371840
355.220626	1855.851710	18.184474	-0.066599	2.366995
355.237178	1847.896444	18.189479	-0.066597	2.362172
355.353765	1839.923821	18.194483	-0.066613	2.357336
354.782768	1832.065765	18.199488	-0.066502	2.352503
355.042326	1824.016156	18.204493	-0.066545	2.347612
355.161500	1816.030316	18.209498	-0.066562	2.342738
355.230196	1808.080107	18.214503	-0.066569	2.337871
355.278515	1800.105757	18.219507	-0.066573	2.332978
355.215079	1792.159586	18.224512	-0.066556	2.328083
355.389235	1784.183694	18.229517	-0.066583	2.323179
354.847399	1776.347243	18.234522	-0.066477	2.318290
354.839320	1768.408501	18.239527	-0.066470	2.313372
354.505734	1760.490223	18.244531	-0.066403	2.308429
354.494723	1752.498285	18.249536	-0.066396	2.303458
354.353477	1744.582346	18.254541	-0.066364	2.298511
354.353327	1736.593889	18.259546	-0.066359	2.293521
354.261361	1728.647466	18.264551	-0.066337	2.288538
354.408298	1720.656216	18.269555	-0.066359	2.283537
354.300397	1712.726648	18.274560	-0.066333	2.278542
354.131165	1704.812412	18.279565	-0.066297	2.273540
353.983289	1696.792243	18.284570	-0.066264	2.268462
354.203953	1688.799366	18.289575	-0.066300	2.263422
354.052312	1680.889101	18.294579	-0.066266	2.258390
353.798750	1672.966655	18.299584	-0.066214	2.253331
353.834377	1665.010935	18.304589	-0.066215	2.248264
353.868373	1657.034521	18.309594	-0.066216	2.243173
353.764595	1649.139840	18.314599	-0.066192	2.238110
353.364056	1641.248393	18.319603	-0.066112	2.233011
353.094101	1633.316617	18.324608	-0.066057	2.227886
353.300118	1625.316860	18.329613	-0.066090	2.222748
353.053735	1617.409154	18.334618	-0.066039	2.217617
353.236378	1609.411145	18.339623	-0.066067	2.212454
353.025314	1601.502485	18.344627	-0.066023	2.207302
352.795707	1593.569757	18.349632	-0.065975	2.202120
352.743738	1585.648107	18.354637	-0.065960	2.196949
352.515826	1577.695220	18.359642	-0.065912	2.191729
352.351805	1569.751625	18.364647	-0.065877	2.186509
352.461224	1561.775814	18.369651	-0.065892	2.181281
352.216908	1553.861425	18.374656	-0.065841	2.176047
352.640010	1545.830289	18.379661	-0.065915	2.170787
352.646069	1537.879110	18.384666	-0.065911	2.165527
352.738814	1529.944216	18.389671	-0.065923	2.160274
352.730139	1522.025960	18.394675	-0.065916	2.155009
352.191662	1514.188135	18.399680	-0.065810	2.149734
352.426201	1506.183411	18.404685	-0.065849	2.144409
352.083618	1498.290772	18.409690	-0.065780	2.139090
351.804621	1490.397221	18.414695	-0.065723	2.133764
352.061696	1482.383190	18.419699	-0.065765	2.128394
351.965442	1474.449478	18.424704	-0.065742	2.123031
352.446513	1466.443092	18.429709	-0.065826	2.117662
352.394834	1458.506022	18.434714	-0.065812	2.112274
351.831087	1450.657567	18.439719	-0.065701	2.106882
351.942251	1442.684889	18.444723	-0.065717	2.101458
351.805750	1434.760284	18.449728	-0.065686	2.096028
351.525641	1426.892460	18.454733	-0.065629	2.090609
351.209310	1418.962017	18.459738	-0.065565	2.085129
351.022477	1411.076273	18.464743	-0.065525	2.079678
351.222539	1403.079121	18.469747	-0.065557	2.074175
351.055040	1395.156171	18.474752	-0.065520	2.068671
351.244987	1387.182011	18.479757	-0.065551	2.063153
351.165738	1379.270108	18.484762	-0.065531	2.057637
350.915284	1371.380292	18.489767	-0.065479	2.052104
351.124061	1363.385746	18.494771	-0.065512	2.046529
351.059965	1355.478116	18.499776	-0.065495	2.040972
350.488353	1347.676042	18.504781	-0.065384	2.035422
350.460190	1339.696958	18.509786	-0.065373	2.029788
350.675018	1331.702743	18.514791	-0.065408	2.024153
351.140281	1323.706661	18.519795	-0.065489	2.018527
350.495967	1315.890098	18.524800	-0.065364	2.012896
350.946885	1307.883378	18.529805	-0.065443	2.007230
350.920657	1299.965066	18.534810	-0.065433	2.001560
350.701850	1292.098084	18.539815	-0.065387	1.995891
350.640278	1284.180561	18.544819	-0.065370	1.990185
350.250485	1276.317932	18.549824	-0.065293	1.984468
350.015167	1268.452569	18.554829	-0.065244	1.978748
350.330024	1260.419321	18.559834	-0.065297	1.972950
350.512736	1252.469023	18.564839	-0.065326	1.967181
350.560000	1244.564332	18.569843	-0.065329	1.961414
350.773731	1236.613541	18.574848	-0.065364	1.955613
351.112169	1228.669698	18.579853	-0.065422	1.949815
350.519224	1220.847408	18.584858	-0.065306	1.943986
350.071719	1213.013816	18.589863	-0.065218	1.938147
350.016425	1205.076805	18.594867	-0.065202	1.932257
349.944057	1197.137453	18.599872	-0.065183	1.926345
349.630419	1189.290801	18.604877	-0.065120	1.920457
349.720127	1181.317913	18.609882	-0.065131	1.914503
349.944671	1173.369393	18.614887	-0.065168	1.908563
349.375870	1165.557499	18.619891	-0.065057	1.902617
349.145213	1157.655241	18.624896	-0.065009	1.896623
348.922754	1149.768650	18.629901	-0.064962	1.890622
349.045791	1141.794450	18.634906	-0.064980	1.884576
349.541863	1133.806080	18.639911	-0.065067	1.878543
349.351451	1125.939966	18.644915	-0.065026	1.872504
349.312986	1118.022470	18.649920	-0.065014	1.866424
349.316040	1110.129057	18.654925	-0.065009	1.860347
348.886752	1102.292871	18.659930	-0.064924	1.854243
349.105781	1094.333088	18.664935	-0.064960	1.848101
348.930778	1086.473412	18.669939	-0.064922	1.841969
348.746876	1078.596052	18.674944	-0.064883	1.835801
348.920897	1070.651239	18.679949	-0.064910	1.829603
348.710223	1062.780678	18.684954	-0.064865	1.823395
348.354202	1054.954806	18.689959	-0.064794	1.817184
348.165116	1047.069229	18.694963	-0.064754	1.810925
348.172697	1039.124783	18.699968	-0.064750	1.804621
348.227062	1031.249502	18.704973	-0.064755	1.798356
348.026484	1023.353845	18.709978	-0.064712	1.792021
348.166887	1015.395678	18.714983	-0.064733	1.785656
348.290511	1007.493102	18.719987	-0.064751	1.779311
348.220721	999.610727	18.724992	-0.064733	1.772935
348.360383	991.684407	18.729997	-0.064754	1.766528
348.335565	983.812583	18.735002	-0.064744	1.760120
348.599411	975.907595	18.740007	-0.064788	1.753698
348.418397	968.058610	18.745011	-0.064749	1.747242
348.011730	960.248989	18.750016	-0.064668	1.740765
347.513021	952.486448	18.755021	-0.064570	1.734291
347.649186	944.526341	18.760026	-0.064590	1.727711
347.223563	936.720833	18.765031	-0.064506	1.721162
347.394364	928.797593	18.770035	-0.064532	1.714567
347.481878	920.875210	18.775040	-0.064543	1.707936
347.083821	913.068186	18.780045	-0.064464	1.701312
347.334966	905.131970	18.785050	-0.064506	1.694640
347.076725	897.288704	18.790055	-0.064452	1.687952
347.501395	889.341096	18.795059	-0.064526	1.681241
347.196822	881.546791	18.800064	-0.064465	1.674535
347.317786	873.655839	18.805069	-0.064482	1.667777
347.180741	865.804523	18.810074	-0.064451	1.660990
347.099537	857.964411	18.815079	-0.064431	1.654193
346.565456	850.187976	18.820083	-0.064326	1.647360
346.829661	842.247986	18.825088	-0.064370	1.640467
346.719240	834.424608	18.830093	-0.064345	1.633595
346.126331	826.622125	18.835098	-0.064229	1.626644
346.247096	818.720397	18.840103	-0.064246	1.619676
345.897803	810.933398	18.845107	-0.064176	1.612714
345.754455	803.063888	18.850112	-0.064144	1.605676
346.322872	795.117338	18.855117	-0.064245	1.598642
346.383847	787.239754	18.860122	-0.064251	1.591565
345.879617	779.490158	18.865127	-0.064152	1.584490
345.878896	771.657245	18.870131	-0.064147	1.577381
345.679480	763.826272	18.875136	-0.064105	1.570212
345.858464	755.960407	18.880141	-0.064133	1.563035
345.768472	748.131339	18.885146	-0.064111	1.555818
345.649829	740.314286	18.890151	-0.064084	1.548574
346.000184	732.393762	18.895155	-0.064144	1.541271
345.560948	724.645249	18.900160	-0.064057	1.533974
345.891856	716.757101	18.905165	-0.064113	1.526628
345.881423	708.944417	18.910170	-0.064106	1.519266
345.868676	701.141773	18.915175	-0.064099	1.511877
345.862622	693.327979	18.920179	-0.064092	1.504443
345.482196	685.580917	18.925184	-0.064016	1.496976
345.494098	677.756901	18.930189	-0.064014	1.489460
345.349336	669.969743	18.935194	-0.063981	1.481917
345.377966	662.149089	18.940199	-0.063982	1.474329
345.453406	654.300702	18.945203	-0.063991	1.466683
344.891666	646.589645	18.950208	-0.063881	1.459029
344.710481	638.811942	18.955213	-0.063842	1.451331
344.566719	631.008514	18.960218	-0.063810	1.443572
344.495920	623.227406	18.965223	-0.063792	1.435805
344.549553	615.418867	18.970227	-0.063797	1.427989
344.488985	607.618957	18.975232	-0.063780	1.420120
344.575677	599.833995	18.980237	-0.063791	1.412247
344.226287	592.097025	18.985242	-0.063721	1.404304
344.393752	584.288546	18.990247	-0.063747	1.396331
344.066018	576.569644	18.995251	-0.063681	1.388320
343.991337	568.782157	19.000256	-0.063662	1.380235
344.649934	560.893889	19.005261	-0.063779	1.372125
344.437903	553.163976	19.010266	-0.063735	1.363980
343.832039	545.537308	19.015271	-0.063617	1.355826
343.762098	537.787854	19.020275	-0.063599	1.347587
343.996315	529.972251	19.025280	-0.063637	1.339281
343.988664	522.233309	19.030285	-0.063631	1.330962
344.255404	514.436935	19.035290	-0.063675	1.322579
343.809781	506.791867	19.040295	-0.063587	1.314176
343.891801	498.949439	19.045299	-0.063598	1.305600
343.827527	491.235079	19.050304	-0.063581	1.297082
343.530487	483.571364	19.055309	-0.063520	1.288520
343.607427	475.825731	19.060314	-0.063529	1.279880
343.224103	468.195802	19.065319	-0.063453	1.271224
343.709577	460.390941	19.070323	-0.063538	1.262476
343.879216	452.657643	19.075328	-0.063565	1.253688
343.724925	445.002931	19.080333	-0.063531	1.244866
343.349955	437.396196	19.085338	-0.063456	1.235993
343.357188	429.708494	19.090343	-0.063453	1.227036
343.130137	422.071080	19.095347	-0.063405	1.218027
342.874172	414.416013	19.100352	-0.063353	1.208923
343.078970	406.712248	19.105357	-0.063386	1.199785
342.672917	399.131477	19.110362	-0.063305	1.190600
342.739188	391.447470	19.115367	-0.063312	1.181316
342.948472	383.764517	19.120371	-0.063346	1.171990
342.588582	376.190681	19.125376	-0.063274	1.162604
342.436586	368.591532	19.130381	-0.063241	1.153154
342.714257	360.875756	19.135386	-0.063288	1.143571
342.468851	353.310152	19.140391	-0.063237	1.133985
342.212316	345.743154	19.145395	-0.063184	1.124312
342.217513	338.135629	19.150400	-0.063180	1.114561
342.317892	330.527026	19.155405	-0.063194	1.104743
342.379636	322.931417	19.160410	-0.063200	1.094846
341.803206	315.465567	19.165415	-0.063088	1.084885
341.271727	308.008642	19.170419	-0.062984	1.074853
341.427781	300.399019	19.175424	-0.063008	1.064681
341.343703	292.863737	19.180429	-0.062988	1.054456
341.565182	285.266905	19.185434	-0.063024	1.044119
340.838219	277.890068	19.190439	-0.062884	1.033755
341.219383	270.299054	19.195443	-0.062950	1.023255
340.757566	262.879456	19.200448	-0.062859	1.012682
340.720258	255.402141	19.205453	-0.062847	1.002021
340.406192	247.977385	19.210458	-0.062784	0.991251
340.833128	240.400162	19.215463	-0.062858	0.980328
341.242967	232.872481	19.220467	-0.062929	0.969352
341.117810	225.471814	19.225472	-0.062901	0.958300
340.964317	218.113360	19.230477	-0.062868	0.947175
340.786968	210.744132	19.235482	-0.062830	0.935896
340.708396	203.379943	19.240487	-0.062811	0.924513
340.892181	195.998659	19.245491	-0.062840	0.913034
339.962534	188.820135	19.250496	-0.062662	0.901420
339.964072	181.487191	19.255501	-0.062658	0.889669
340.161020	174.132483	19.260506	-0.062689	0.877782
340.055062	166.867955	19.265511	-0.062665	0.865792
339.755925	159.668664	19.270515	-0.062604	0.853686
339.821946	152.408106	19.275520	-0.062612	0.841412
339.951022	145.163281	19.280525	-0.062631	0.829002
339.921646	137.964987	19.285530	-0.062621	0.816436
340.205811	130.744330	19.290535	-0.062669	0.803733
340.047345	123.661298	19.295539	-0.062635	0.790933
340.374693	116.490919	19.300544	-0.062691	0.777921
339.779112	109.548761	19.305549	-0.062576	0.764808
339.307859	102.594576	19.310554	-0.062483	0.751485
339.427914	95.547056	19.315559	-0.062501	0.737945
339.162308	88.633180	19.320563	-0.062447	0.724280
339.095992	81.704406	19.325568	-0.062430	0.710393
338.359289	75.126788	19.330573	-0.062289	0.696707