Mon Apr 19 09:06:17 2021

Number of Points = 3625
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
4.121035	0.098363	0.000000	0.000150	0.306524

3.931890	0.187794	0.005005	0.000185	0.306783
4.520674	0.074529	0.010010	0.000075	0.306753
4.827766	0.017532	0.015014	0.000018	0.306748
4.369089	0.104297	0.020019	0.000104	0.306764
4.319801	0.112291	0.025024	0.000113	0.306759
4.247972	0.128608	0.030029	0.000126	0.306774
3.938598	0.183914	0.035034	0.000184	0.306770
4.199141	0.136599	0.040038	0.000135	0.306770
4.389465	0.080329	0.045043	0.000100	0.306667
4.612945	-0.013874	0.050048	0.000058	0.306414
4.681799	-0.025040	0.055053	0.000046	0.306420
4.636348	-0.018784	0.060058	0.000054	0.306410
4.609135	-0.013411	0.065062	0.000059	0.306412
4.873134	-0.062094	0.070067	0.000010	0.306409
4.284257	0.047264	0.075072	0.000120	0.306420
4.220363	0.062934	0.080077	0.000132	0.306439
3.865018	0.127156	0.085082	0.000198	0.306437
3.911966	0.119445	0.090086	0.000189	0.306440
3.942806	0.114100	0.095091	0.000184	0.306441
3.982982	0.104132	0.100096	0.000176	0.306429
4.092516	0.036679	0.105101	0.000156	0.306204
3.835264	0.067690	0.110106	0.000204	0.306129
4.306711	-0.020960	0.115110	0.000116	0.306115
4.364375	-0.031019	0.120115	0.000105	0.306117
4.080756	0.019898	0.125120	0.000158	0.306114
3.933034	0.052158	0.130125	0.000186	0.306139
4.148369	0.007344	0.135130	0.000146	0.306112
4.499254	-0.123002	0.140134	0.000080	0.305797
4.774483	-0.176388	0.145139	0.000029	0.305781
4.537934	-0.134468	0.150144	0.000073	0.305776
5.006146	-0.219580	0.155149	-0.000014	0.305775
4.560389	-0.169611	0.160154	0.000069	0.305628
4.550023	-0.189153	0.165158	0.000071	0.305527
4.872503	-0.248923	0.170163	0.000011	0.305521
4.548467	-0.188764	0.175168	0.000072	0.305527
4.646800	-0.261222	0.180173	0.000053	0.305268
4.019061	-0.162153	0.185178	0.000170	0.305197
3.647279	-0.091002	0.190182	0.000239	0.305213
3.582668	-0.078321	0.195187	0.000252	0.305218
3.520481	-0.114407	0.200192	0.000263	0.304993
3.776371	-0.183261	0.205197	0.000216	0.304887
3.858846	-0.201283	0.210202	0.000200	0.304872
4.015172	-0.227841	0.215206	0.000171	0.304881
4.046456	-0.302109	0.220211	0.000166	0.304555
4.189742	-0.332670	0.225216	0.000139	0.304533
4.127383	-0.317738	0.230221	0.000151	0.304550
3.659092	-0.281712	0.235226	0.000238	0.304317
4.079898	-0.368791	0.240230	0.000159	0.304266
4.055080	-0.362966	0.245235	0.000164	0.304272
3.571451	-0.333040	0.250240	0.000254	0.303996
3.736959	-0.372553	0.255245	0.000223	0.303951
3.583441	-0.345999	0.260250	0.000252	0.303944
3.443958	-0.375221	0.265254	0.000278	0.303684
3.859550	-0.461971	0.270259	0.000201	0.303631
3.599886	-0.423393	0.275264	0.000249	0.303589
3.571203	-0.475299	0.280269	0.000255	0.303317
3.694061	-0.500093	0.285274	0.000232	0.303305
3.901473	-0.569794	0.290278	0.000193	0.303152
3.776085	-0.574729	0.295283	0.000217	0.303019
4.042587	-0.634808	0.300288	0.000167	0.302964
3.805089	-0.651038	0.305293	0.000211	0.302680
4.147205	-0.718304	0.310298	0.000148	0.302655
4.414446	-0.824712	0.315302	0.000098	0.302378
4.427823	-0.834981	0.320307	0.000096	0.302340
4.111760	-0.833573	0.325312	0.000155	0.302072
4.001851	-0.822554	0.330317	0.000175	0.302029
3.844472	-0.837984	0.335322	0.000204	0.301818
4.358775	-0.951722	0.340326	0.000109	0.301720
4.213636	-0.976316	0.345331	0.000136	0.301476
4.042173	-0.962885	0.350336	0.000168	0.301390
4.235130	-1.049238	0.355341	0.000132	0.301144
4.085299	-1.033738	0.360346	0.000160	0.301087
4.118484	-1.104642	0.365350	0.000154	0.300775
4.472999	-1.179741	0.370355	0.000088	0.300724
4.111628	-1.154491	0.375360	0.000155	0.300529
4.572186	-1.271852	0.380365	0.000070	0.300367
4.151742	-1.234814	0.385370	0.000148	0.300177
3.972885	-1.251587	0.390374	0.000181	0.299939
3.660470	-1.209002	0.395379	0.000239	0.299870
3.578071	-1.261897	0.400384	0.000255	0.299542
3.926675	-1.341634	0.405389	0.000190	0.299463
2.977558	-1.207786	0.410394	0.000367	0.299276
2.951764	-1.237768	0.415398	0.000372	0.299108
3.001203	-1.279956	0.420403	0.000362	0.298947
2.957009	-1.320188	0.425408	0.000371	0.298713
3.588836	-1.457563	0.430413	0.000253	0.298604
3.446116	-1.495942	0.435418	0.000280	0.298292
3.032989	-1.442372	0.440422	0.000357	0.298187
3.025903	-1.474663	0.445427	0.000358	0.298024
2.706201	-1.469901	0.450432	0.000418	0.297765
2.792213	-1.506591	0.455437	0.000402	0.297662
2.351576	-1.486260	0.460442	0.000484	0.297371
2.004479	-1.448601	0.465446	0.000548	0.297248
2.061985	-1.501438	0.470451	0.000538	0.297041
1.951405	-1.521346	0.475456	0.000558	0.296846
1.553100	-1.464131	0.480461	0.000633	0.296772
1.388182	-1.498031	0.485466	0.000663	0.296460
1.641912	-1.561743	0.490470	0.000616	0.296374
1.760866	-1.635127	0.495475	0.000594	0.296121
1.648714	-1.649364	0.500480	0.000615	0.295951
2.026582	-1.749762	0.505485	0.000545	0.295796
1.890576	-1.775079	0.510490	0.000570	0.295551
1.512356	-1.731987	0.515494	0.000641	0.295425
1.279760	-1.730438	0.520499	0.000684	0.295225
1.426972	-1.810336	0.525504	0.000657	0.294964
0.964033	-1.748454	0.530509	0.000743	0.294855
1.247427	-1.860959	0.535514	0.000690	0.294555
1.176856	-1.882002	0.540518	0.000703	0.294389
1.153521	-1.905125	0.545523	0.000708	0.294254
0.791878	-1.907003	0.550528	0.000775	0.293921
0.892067	-1.948537	0.555533	0.000757	0.293806
0.903373	-1.988399	0.560538	0.000755	0.293620
1.264679	-2.117243	0.565542	0.000687	0.293308
1.308773	-2.153724	0.570547	0.000679	0.293167
1.453417	-2.222457	0.575552	0.000652	0.292957
1.142414	-2.227455	0.580557	0.000710	0.292653
1.111242	-2.262574	0.585562	0.000716	0.292451
1.266451	-2.329570	0.590566	0.000687	0.292259
0.405469	-2.219333	0.595571	0.000848	0.292030
-0.109691	-2.175984	0.600576	0.000944	0.291780
0.630688	-2.340987	0.605581	0.000806	0.291629
1.240518	-2.501815	0.610586	0.000693	0.291381
0.328980	-2.395693	0.615590	0.000862	0.291085
-0.283681	-2.319080	0.620595	0.000976	0.290912
-0.206306	-2.369437	0.625600	0.000962	0.290731
-0.118200	-2.427967	0.630605	0.000946	0.290519
-0.662864	-2.375635	0.635610	0.001047	0.290286
-0.882045	-2.368679	0.640614	0.001088	0.290122
-0.917180	-2.413280	0.645619	0.001095	0.289867
-1.196798	-2.410737	0.650624	0.001147	0.289626
-0.636025	-2.544945	0.655629	0.001042	0.289464
-0.888200	-2.542472	0.660634	0.001089	0.289247
-1.042655	-2.572030	0.665638	0.001118	0.288959
-1.449816	-2.533254	0.670643	0.001194	0.288782
-1.584583	-2.547631	0.675648	0.001219	0.288587
-1.690743	-2.584025	0.680653	0.001239	0.288307
-1.925960	-2.574478	0.685658	0.001283	0.288140
-2.222076	-2.551644	0.690662	0.001338	0.287984
-2.518216	-2.561159	0.695667	0.001393	0.287666
-2.463219	-2.608154	0.700672	0.001383	0.287479
-3.770933	-2.395767	0.705677	0.001626	0.287351
-3.336924	-2.531049	0.710682	0.001546	0.287067
-3.043263	-2.610837	0.715686	0.001491	0.286934
-3.502313	-2.567292	0.720691	0.001577	0.286732
-4.091081	-2.506052	0.725696	0.001686	0.286501
-4.556509	-2.438511	0.730701	0.001773	0.286414
-4.714867	-2.471779	0.735706	0.001802	0.286100
-4.513261	-2.527309	0.740710	0.001765	0.286005
-4.591947	-2.559668	0.745715	0.001780	0.285768
-5.477832	-2.424670	0.750720	0.001945	0.285636
-5.578430	-2.429755	0.755725	0.001963	0.285517
-5.477675	-2.500317	0.760730	0.001945	0.285252
-6.060633	-2.407258	0.765734	0.002053	0.285186
-6.492895	-2.386007	0.770739	0.002134	0.284895
-7.044037	-2.290732	0.775744	0.002236	0.284870
-7.047540	-2.347291	0.780749	0.002237	0.284579
-7.231377	-2.318739	0.785754	0.002271	0.284554
-7.501929	-2.322252	0.790758	0.002322	0.284285
-7.888583	-2.253482	0.795763	0.002394	0.284277
-8.125052	-2.267729	0.800768	0.002438	0.283986
-8.444385	-2.219060	0.805773	0.002497	0.283938
-8.524325	-2.239224	0.810778	0.002512	0.283760
-8.724995	-2.227161	0.815782	0.002550	0.283636
-9.019323	-2.196638	0.820787	0.002604	0.283518
-9.594896	-2.134549	0.825792	0.002712	0.283301
-9.509505	-2.145617	0.830797	0.002696	0.283323
-8.879661	-2.319026	0.835802	0.002579	0.283022
-9.451803	-2.215439	0.840806	0.002685	0.283019
-9.579994	-2.241234	0.845811	0.002709	0.282768
-10.223779	-2.142154	0.850816	0.002829	0.282676
-10.060171	-2.194766	0.855821	0.002798	0.282558
-10.310924	-2.186816	0.860826	0.002845	0.282365
-10.173182	-2.214596	0.865830	0.002820	0.282351
-10.143528	-2.281388	0.870835	0.002814	0.282036
-10.248094	-2.268088	0.875840	0.002834	0.282006
-9.906433	-2.371965	0.880845	0.002770	0.281792
-9.994974	-2.371301	0.885850	0.002787	0.281712
-11.029348	-2.220447	0.890854	0.002979	0.281521
-10.984995	-2.250335	0.895859	0.002971	0.281408
-10.655908	-2.334003	0.900864	0.002910	0.281286
-11.206208	-2.269361	0.905869	0.003012	0.281103
-11.917908	-2.139973	0.910874	0.003145	0.281103
-11.771715	-2.226053	0.915878	0.003118	0.280796
-11.473610	-2.284654	0.920883	0.003062	0.280773
-12.060992	-2.203720	0.925888	0.003172	0.280640
-12.517246	-2.135771	0.930893	0.003257	0.280562
-12.128474	-2.215195	0.935898	0.003184	0.280517
-12.755121	-2.162408	0.940902	0.003301	0.280201
-13.220488	-2.073029	0.945907	0.003388	0.280225
-13.041821	-2.135200	0.950912	0.003354	0.280072
-13.179497	-2.142105	0.955917	0.003380	0.279906
-13.166622	-2.145550	0.960922	0.003378	0.279900
-12.973523	-2.238905	0.965926	0.003342	0.279599
-13.395986	-2.165553	0.970931	0.003421	0.279581
-13.973947	-2.079987	0.975936	0.003528	0.279479
-13.976315	-2.116618	0.980941	0.003529	0.279287
-14.148616	-2.082960	0.985946	0.003561	0.279299
-14.174900	-2.124164	0.990950	0.003566	0.279060
-14.566833	-2.074270	0.995955	0.003639	0.278949
-14.531099	-2.079819	1.000960	0.003632	0.278954
-14.271131	-2.183726	1.005965	0.003584	0.278660
-15.074533	-2.040554	1.010970	0.003733	0.278644
-14.997745	-2.069277	1.015974	0.003719	0.278567
-15.464903	-2.025727	1.020979	0.003806	0.278352
-15.688141	-1.990084	1.025984	0.003848	0.278326
-15.420229	-2.054200	1.030989	0.003798	0.278246
-16.017642	-1.981867	1.035994	0.003909	0.278056
-15.739384	-2.035994	1.040998	0.003857	0.278038
-15.791367	-2.053459	1.046003	0.003867	0.277898
-16.190439	-2.020335	1.051008	0.003941	0.277692
-16.309222	-1.994369	1.056013	0.003964	0.277714
-15.663670	-2.153421	1.061018	0.003843	0.277497
-15.944855	-2.126145	1.066022	0.003896	0.277372
-15.822397	-2.152875	1.071027	0.003873	0.277349
-16.647979	-2.061309	1.076032	0.004027	0.277043
-16.833221	-2.024089	1.081037	0.004061	0.277061
-15.699914	-2.256227	1.086042	0.003850	0.276925
-17.045955	-2.042441	1.091046	0.004101	0.276762
-16.786719	-2.090446	1.096051	0.004053	0.276758
-16.554060	-2.181994	1.101056	0.004010	0.276500
-16.740729	-2.163593	1.106061	0.004044	0.276418
-16.858213	-2.155250	1.111066	0.004066	0.276350
-17.468487	-2.090844	1.116070	0.004180	0.276105
-17.369031	-2.104567	1.121075	0.004161	0.276128
-17.847910	-2.052453	1.126080	0.004251	0.275944
-17.808523	-2.085774	1.131085	0.004243	0.275807
-17.627914	-2.121178	1.136090	0.004210	0.275793
-18.037323	-2.083689	1.141094	0.004286	0.275599
-18.369286	-2.028437	1.146099	0.004348	0.275572
-17.801742	-2.147635	1.151104	0.004242	0.275488
-17.635459	-2.234539	1.156109	0.004211	0.275190
-18.544699	-2.064265	1.161114	0.004381	0.275215
-19.006323	-2.011300	1.166118	0.004467	0.275052
-19.088277	-2.021221	1.171123	0.004482	0.274921
-19.436972	-1.959271	1.176128	0.004547	0.274913
-19.412873	-2.005532	1.181133	0.004542	0.274692
-19.563268	-1.999051	1.186138	0.004570	0.274582
-18.963987	-2.111903	1.191142	0.004459	0.274561
-19.409864	-2.078158	1.196147	0.004542	0.274312
-19.500246	-2.069760	1.201152	0.004559	0.274269
-19.281822	-2.126950	1.206157	0.004518	0.274176
-19.797681	-2.078221	1.211162	0.004614	0.273938
-19.583138	-2.117295	1.216166	0.004574	0.273938
-19.538959	-2.161340	1.221171	0.004566	0.273747
-20.219491	-2.059449	1.226176	0.004693	0.273631
-20.151034	-2.073032	1.231181	0.004680	0.273625
-20.371748	-2.090194	1.236186	0.004721	0.273321
-20.736620	-2.022675	1.241190	0.004789	0.273327
-20.616954	-2.060192	1.246195	0.004767	0.273244
-21.335824	-1.968575	1.251200	0.004901	0.273036
-21.303876	-1.972297	1.256205	0.004895	0.273047
-21.068285	-2.042580	1.261210	0.004851	0.272901
-21.211872	-2.057537	1.266214	0.004878	0.272683
-21.025287	-2.088039	1.271219	0.004843	0.272701
-21.613427	-2.026449	1.276224	0.004953	0.272460
-22.159733	-1.939137	1.281229	0.005055	0.272396
-21.702913	-2.025416	1.286234	0.004970	0.272378
-21.504996	-2.117811	1.291238	0.004933	0.272078
-21.758761	-2.074807	1.296243	0.004980	0.272061
-22.762391	-1.897742	1.301248	0.005167	0.272032
-22.408552	-2.009573	1.306253	0.005101	0.271779
-22.668429	-1.962377	1.311258	0.005150	0.271778
-22.992174	-1.919918	1.316262	0.005210	0.271691
-22.262739	-2.102159	1.321267	0.005074	0.271426
-22.083117	-2.139722	1.326272	0.005041	0.271400
-22.744195	-2.055100	1.331277	0.005164	0.271209
-22.652330	-2.089418	1.336282	0.005147	0.271115
-22.839799	-2.059503	1.341286	0.005182	0.271093
-23.092886	-2.066197	1.346291	0.005229	0.270811
-23.680055	-1.959955	1.351296	0.005338	0.270808
-23.656717	-1.975742	1.356301	0.005334	0.270746
-23.961471	-1.953149	1.361306	0.005391	0.270570
-24.132584	-1.923870	1.366310	0.005423	0.270560
-23.793668	-2.010729	1.371315	0.005360	0.270425
-24.201349	-1.976448	1.376320	0.005436	0.270211
-24.439741	-1.929876	1.381325	0.005480	0.270228
-24.628264	-1.926558	1.386330	0.005515	0.270062
-24.559196	-1.970670	1.391334	0.005502	0.269892
-24.360545	-2.005438	1.396339	0.005465	0.269899
-24.651753	-1.999795	1.401344	0.005520	0.269645
-24.784091	-1.987771	1.406349	0.005544	0.269580
-25.022924	-1.944485	1.411354	0.005589	0.269579
-25.908193	-1.833891	1.416358	0.005754	0.269308
-25.790553	-1.853767	1.421363	0.005732	0.269316
-25.655979	-1.880157	1.426368	0.005707	0.269305
-26.154039	-1.843924	1.431373	0.005800	0.269013
-26.231648	-1.837888	1.436378	0.005814	0.268969
-26.003497	-1.879973	1.441382	0.005772	0.268966
-25.948595	-1.935707	1.446387	0.005761	0.268719
-26.647984	-1.820372	1.451392	0.005892	0.268655
-26.570857	-1.833420	1.456397	0.005877	0.268660
-26.338511	-1.923524	1.461402	0.005834	0.268402
-26.734675	-1.865843	1.466406	0.005908	0.268324
-26.047370	-1.992901	1.471411	0.005780	0.268313
-26.299801	-1.997883	1.476416	0.005827	0.268038
-25.835553	-2.088121	1.481421	0.005741	0.268006
-26.326341	-2.024271	1.486426	0.005832	0.267869
-26.627217	-2.005495	1.491430	0.005888	0.267674
-26.514863	-2.023414	1.496435	0.005867	0.267687
-27.208032	-1.948788	1.501440	0.005996	0.267409
-27.284184	-1.941642	1.506445	0.006011	0.267372
-26.896051	-2.023631	1.511450	0.005938	0.267310
-27.789499	-1.909954	1.516454	0.006105	0.267045
-27.680656	-1.927568	1.521459	0.006085	0.267057
-27.098184	-2.062014	1.526464	0.005976	0.266902
-27.596186	-1.999253	1.531469	0.006069	0.266751
-27.778947	-1.963750	1.536474	0.006103	0.266763
-27.778988	-2.019678	1.541478	0.006103	0.266459
-27.417673	-2.093050	1.546483	0.006036	0.266417
-27.859006	-2.038267	1.551488	0.006118	0.266278
-28.267425	-1.995570	1.556493	0.006194	0.266106
-27.980854	-2.046488	1.561498	0.006141	0.266113
-28.657451	-1.974123	1.566502	0.006267	0.265836
-28.834697	-1.946163	1.571507	0.006300	0.265813
-28.544294	-2.012222	1.576512	0.006246	0.265741
-28.662089	-2.029187	1.581517	0.006268	0.265531
-29.183738	-1.930018	1.586522	0.006365	0.265554
-29.472068	-1.914044	1.591526	0.006419	0.265355
-29.427323	-1.947705	1.596531	0.006410	0.265215
-29.955588	-1.851985	1.601536	0.006509	0.265213
-29.752983	-1.934690	1.606541	0.006471	0.264962
-30.098105	-1.881133	1.611546	0.006535	0.264912
-30.579203	-1.792076	1.616550	0.006625	0.264920
-30.277063	-1.905105	1.621555	0.006569	0.264602
-30.439936	-1.881463	1.626560	0.006599	0.264569
-30.278685	-1.917400	1.631565	0.006569	0.264533
-31.000953	-1.827947	1.636570	0.006704	0.264303
-30.782930	-1.869497	1.641574	0.006663	0.264292
-30.441463	-1.951545	1.646579	0.006600	0.264183
-31.240143	-1.847801	1.651584	0.006748	0.263955
-30.959338	-1.900044	1.656589	0.006696	0.263948
-30.720113	-1.975663	1.661594	0.006652	0.263772
-31.285688	-1.899390	1.666598	0.006757	0.263626
-31.183518	-1.915687	1.671603	0.006738	0.263638
-31.206330	-1.966390	1.676608	0.006742	0.263336
-31.379819	-1.941487	1.681613	0.006775	0.263299
-31.583059	-1.917516	1.686618	0.006813	0.263228
-31.635387	-1.948481	1.691622	0.006822	0.263005
-31.516411	-1.966392	1.696627	0.006800	0.263025
-32.090184	-1.905962	1.701632	0.006907	0.262783
-32.805482	-1.792688	1.706637	0.007040	0.262690
-32.510726	-1.844990	1.711642	0.006985	0.262697
-32.282289	-1.938800	1.716646	0.006943	0.262408
-32.562303	-1.892521	1.721651	0.006995	0.262382
-32.875348	-1.843708	1.726656	0.007053	0.262337
-33.014419	-1.869267	1.731661	0.007079	0.262056
-32.922908	-1.886408	1.736666	0.007062	0.262053
-33.408637	-1.817853	1.741670	0.007153	0.261943
-33.349605	-1.857508	1.746675	0.007142	0.261783
-33.376370	-1.854941	1.751680	0.007147	0.261770
-33.291275	-1.908439	1.756685	0.007131	0.261560
-33.425488	-1.907247	1.761690	0.007156	0.261431
-33.722012	-1.853847	1.766694	0.007211	0.261428
-34.394645	-1.780144	1.771699	0.007337	0.261158
-34.138282	-1.832469	1.776704	0.007289	0.261126
-33.559131	-1.950082	1.781709	0.007181	0.261058
-34.234854	-1.872697	1.786714	0.007307	0.260805
-34.364291	-1.851241	1.791718	0.007331	0.260793
-33.861632	-1.963377	1.796723	0.007238	0.260678
-34.625949	-1.845723	1.801728	0.007380	0.260559
-34.422698	-1.882813	1.806733	0.007342	0.260558
-34.779981	-1.870094	1.811738	0.007409	0.260267
-35.028518	-1.832943	1.816742	0.007455	0.260222
-34.917108	-1.865465	1.821747	0.007434	0.260153
-35.480233	-1.806243	1.826752	0.007539	0.259912
-34.988725	-1.898729	1.831757	0.007448	0.259895
-35.275617	-1.876236	1.836762	0.007501	0.259729
-35.826240	-1.803845	1.841766	0.007604	0.259574
-35.384414	-1.881975	1.846771	0.007522	0.259586
-36.099484	-1.794322	1.851776	0.007655	0.259349
-36.299514	-1.764844	1.856781	0.007692	0.259310
-35.898927	-1.842433	1.861786	0.007617	0.259284
-36.257200	-1.833897	1.866790	0.007684	0.258967
-36.470749	-1.793190	1.871795	0.007724	0.258977
-36.646958	-1.780501	1.876800	0.007757	0.258869
-36.617057	-1.822617	1.881805	0.007751	0.258663
-36.631724	-1.818460	1.886810	0.007754	0.258671
-37.191687	-1.753276	1.891814	0.007858	0.258466
-37.497207	-1.715941	1.896819	0.007915	0.258363
-37.367983	-1.740748	1.901824	0.007891	0.258356
-37.457885	-1.760869	1.906829	0.007908	0.258151
-37.368457	-1.792865	1.911834	0.007891	0.258062
-37.005126	-1.862347	1.916838	0.007824	0.258043
-37.535826	-1.823243	1.921843	0.007923	0.257720
-37.864723	-1.764707	1.926848	0.007984	0.257713
-37.645741	-1.823705	1.931853	0.007943	0.257605
-37.862917	-1.820769	1.936858	0.007984	0.257399
-37.914888	-1.813706	1.941862	0.007993	0.257385
-37.908424	-1.851224	1.946867	0.007992	0.257180
-38.012237	-1.852679	1.951872	0.008012	0.257066
-37.941100	-1.875960	1.956877	0.007999	0.257007
-38.254461	-1.858707	1.961882	0.008057	0.256783
-38.449657	-1.822100	1.966886	0.008093	0.256789
-38.435871	-1.859480	1.971891	0.008091	0.256592
-38.827467	-1.813842	1.976896	0.008164	0.256447
-38.362052	-1.902763	1.981901	0.008077	0.256423
-38.634101	-1.903250	1.986906	0.008128	0.256140
-39.230482	-1.796286	1.991910	0.008239	0.256131
-39.162172	-1.835221	1.996915	0.008226	0.255981
-39.052416	-1.885094	2.001920	0.008206	0.255811

-39.084864	-1.921636	2.011917	0.008212	0.255570
-39.467375	-1.887713	2.021914	0.008283	0.255368
-39.798725	-1.850534	2.031910	0.008345	0.255236
-39.496729	-1.958555	2.041907	0.008289	0.254934
-39.602033	-1.951437	2.051904	0.008309	0.254865
-39.975639	-1.935721	2.061901	0.008378	0.254568
-40.089411	-1.914805	2.071898	0.008399	0.254569
-39.961970	-1.975600	2.081894	0.008376	0.254354
-40.424801	-1.904658	2.091891	0.008462	0.254278
-40.586047	-1.872419	2.101888	0.008492	0.254294
-40.513684	-1.900143	2.111885	0.008479	0.254211
-40.950506	-1.864887	2.121882	0.008560	0.253958
-40.946496	-1.864740	2.131878	0.008560	0.253963
-40.794228	-1.895022	2.141875	0.008531	0.253948
-40.198920	-2.007057	2.151872	0.008421	0.253926
-40.663349	-1.919891	2.161869	0.008507	0.253941
-40.564199	-1.937754	2.171866	0.008489	0.253941
-40.507250	-1.947818	2.181862	0.008478	0.253942
-41.087559	-1.839910	2.191859	0.008586	0.253955
-41.046023	-1.847523	2.201856	0.008579	0.253955
-41.108546	-1.835528	2.211853	0.008590	0.253958
-40.652682	-1.890759	2.221850	0.008506	0.254115
-40.139189	-1.956455	2.231846	0.008410	0.254273
-40.510498	-1.887080	2.241843	0.008479	0.254283
-40.317577	-1.921287	2.251840	0.008443	0.254287
-40.463484	-1.896363	2.261837	0.008471	0.254278
-40.294293	-1.899756	2.271834	0.008439	0.254433
-39.825241	-1.962403	2.281830	0.008352	0.254562
-40.029343	-1.924399	2.291827	0.008390	0.254566
-39.900644	-1.943902	2.301824	0.008366	0.254588
-39.903166	-1.889183	2.311821	0.008367	0.254896
-39.332582	-1.993556	2.321818	0.008261	0.254893
-39.414613	-1.970995	2.331814	0.008276	0.254936
-39.487463	-1.908932	2.341811	0.008290	0.255212
-39.319187	-1.939205	2.351808	0.008258	0.255214
-39.644721	-1.836411	2.361805	0.008319	0.255461
-39.274579	-1.884970	2.371802	0.008250	0.255567
-39.115138	-1.886974	2.381798	0.008221	0.255719
-39.082537	-1.877231	2.391795	0.008215	0.255807
-38.842874	-1.886122	2.401792	0.008170	0.256004
-38.938133	-1.846411	2.411789	0.008188	0.256130
-38.430896	-1.897312	2.421786	0.008093	0.256363
-38.415122	-1.889407	2.431782	0.008091	0.256424
-37.381768	-2.029460	2.441779	0.007898	0.256694
-37.788858	-1.944804	2.451776	0.007974	0.256753
-37.762645	-1.904600	2.461773	0.007969	0.257006
-37.211809	-1.997190	2.471770	0.007867	0.257049
-36.712670	-2.035224	2.481766	0.007774	0.257346
-36.342994	-2.104523	2.491763	0.007705	0.257334
-36.831938	-1.956942	2.501760	0.007796	0.257663
-36.394759	-2.026961	2.511757	0.007715	0.257716
-35.924713	-2.062482	2.521754	0.007628	0.257996
-36.095975	-2.010879	2.531750	0.007660	0.258111
-35.146988	-2.154783	2.541747	0.007483	0.258272
-35.752216	-2.013624	2.551744	0.007596	0.258445
-35.665826	-1.999875	2.561741	0.007580	0.258610
-34.787407	-2.114819	2.571738	0.007416	0.258861
-34.643366	-2.133092	2.581734	0.007390	0.258905
-34.420674	-2.114158	2.591731	0.007348	0.259236
-34.386501	-2.105593	2.601728	0.007342	0.259319
-34.364114	-2.070469	2.611725	0.007338	0.259537
-34.282775	-2.046972	2.621722	0.007323	0.259750
-33.882739	-2.098575	2.631718	0.007248	0.259868
-33.704627	-2.074298	2.641715	0.007215	0.260183
-33.613551	-2.061940	2.651712	0.007198	0.260344
-33.407897	-2.067268	2.661709	0.007160	0.260522
-33.061354	-2.090594	2.671706	0.007096	0.260742
-32.827948	-2.112547	2.681702	0.007052	0.260855
-32.527759	-2.127853	2.691699	0.006997	0.261073
-32.043902	-2.176510	2.701696	0.006907	0.261291
-32.054962	-2.152127	2.711693	0.006909	0.261414
-31.717430	-2.160508	2.721690	0.006846	0.261707
-31.681751	-2.136290	2.731686	0.006839	0.261877
-31.689259	-2.107578	2.741683	0.006841	0.262028
-31.545829	-2.080503	2.751680	0.006814	0.262321
-31.040819	-2.135767	2.761677	0.006720	0.262522
-31.336451	-2.043511	2.771674	0.006775	0.262734
-30.809521	-2.094168	2.781670	0.006677	0.262983
-30.138929	-2.173749	2.791667	0.006553	0.263216
-30.018796	-2.172067	2.801664	0.006530	0.263345
-29.882355	-2.153124	2.811661	0.006505	0.263585
-29.780837	-2.124130	2.821658	0.006486	0.263845
-29.711076	-2.099950	2.831654	0.006473	0.264047
-29.548389	-2.090734	2.841651	0.006443	0.264259
-29.734375	-2.006697	2.851648	0.006478	0.264534
-28.990817	-2.096362	2.861645	0.006339	0.264783
-28.888907	-2.076476	2.871642	0.006320	0.264993
-28.280039	-2.154012	2.881638	0.006207	0.265174
-27.926724	-2.158138	2.891635	0.006142	0.265501
-28.340248	-2.050961	2.901632	0.006219	0.265675
-28.241883	-2.027985	2.911629	0.006200	0.265897
-27.486490	-2.128331	2.921626	0.006060	0.266099
-27.442077	-2.079221	2.931622	0.006052	0.266409
-27.770318	-1.970919	2.941619	0.006113	0.266673
-27.247184	-2.025778	2.951616	0.006015	0.266891
-26.817100	-2.067733	2.961613	0.005935	0.267088
-26.577885	-2.062970	2.971610	0.005891	0.267349
-25.979154	-2.120604	2.981606	0.005780	0.267626
-25.631003	-2.144316	2.991603	0.005715	0.267840
-25.391743	-2.154187	3.001600	0.005670	0.268021
-25.684668	-2.050143	3.011597	0.005725	0.268295
-25.473307	-2.037462	3.021594	0.005686	0.268570
-25.292143	-2.025043	3.031590	0.005652	0.268814
-25.204752	-1.994118	3.041587	0.005636	0.269066
-24.424886	-2.095743	3.051584	0.005491	0.269282
-24.585067	-2.015445	3.061581	0.005521	0.269556
-24.210732	-2.033121	3.071578	0.005451	0.269827
-23.642616	-2.093814	3.081574	0.005345	0.270055
-23.801524	-2.022915	3.091571	0.005375	0.270280
-23.497877	-2.027455	3.101568	0.005318	0.270551
-22.789927	-2.111917	3.111565	0.005187	0.270787
-22.865970	-2.057713	3.121562	0.005201	0.271002
-22.119741	-2.155389	3.131558	0.005062	0.271205
-22.379918	-2.067245	3.141555	0.005111	0.271423
-22.538006	-1.975935	3.151552	0.005140	0.271756
-21.717594	-2.080936	3.161549	0.004987	0.271991
-21.738969	-2.036292	3.171546	0.004992	0.272207
-21.429165	-2.046056	3.181542	0.004934	0.272454
-21.398199	-2.005604	3.191539	0.004928	0.272699
-20.930923	-2.031077	3.201536	0.004841	0.273014
-20.569778	-2.053988	3.211533	0.004774	0.273241
-20.513510	-2.023173	3.221530	0.004764	0.273458
-20.633770	-1.949009	3.231526	0.004786	0.273734
-20.255732	-1.971687	3.241523	0.004716	0.273977
-19.561342	-2.043635	3.251520	0.004587	0.274264
-19.705624	-1.969683	3.261517	0.004614	0.274515
-19.433097	-1.969713	3.271514	0.004563	0.274776
-19.184336	-1.966054	3.281510	0.004517	0.275033
-18.759665	-1.999962	3.291507	0.004438	0.275260
-18.393776	-2.010056	3.301504	0.004370	0.275557
-18.097397	-2.025485	3.311501	0.004315	0.275758
-18.006938	-1.997893	3.321498	0.004298	0.275989
-17.826366	-1.983285	3.331494	0.004264	0.276237
-17.287498	-2.042050	3.341491	0.004164	0.276442
-17.273955	-1.985237	3.351488	0.004162	0.276752
-16.623306	-2.057485	3.361485	0.004041	0.276993
-15.908071	-2.152936	3.371482	0.003907	0.277173
-16.131817	-2.070981	3.381478	0.003949	0.277388
-15.609021	-2.113381	3.391475	0.003852	0.277662
-15.485951	-2.089061	3.401472	0.003829	0.277905
-15.331599	-2.079798	3.411469	0.003800	0.278099
-14.972821	-2.108113	3.421466	0.003734	0.278291
-14.554934	-2.122347	3.431462	0.003656	0.278612
-14.568716	-2.082851	3.441459	0.003659	0.278804
-14.322279	-2.085982	3.451456	0.003613	0.279019
-14.222369	-2.056715	3.461453	0.003594	0.279265
-14.157494	-2.013578	3.471450	0.003582	0.279549
-14.124870	-1.972813	3.481446	0.003576	0.279791
-13.755737	-1.989915	3.491443	0.003508	0.280049
-13.615139	-1.968801	3.501440	0.003481	0.280290
-12.925232	-2.043549	3.511437	0.003353	0.280551
-12.913025	-2.000191	3.521434	0.003351	0.280786
-12.624481	-2.012215	3.531430	0.003297	0.280994
-12.365417	-2.016460	3.541427	0.003249	0.281214
-12.254700	-1.990633	3.551424	0.003229	0.281450
-12.068162	-1.967998	3.561421	0.003194	0.281740
-11.973074	-1.934454	3.571418	0.003176	0.282001
-11.677361	-1.935776	3.581414	0.003121	0.282270
-11.093528	-1.999523	3.591411	0.003013	0.282487
-10.864184	-1.998080	3.601408	0.002970	0.282707
-10.536954	-2.002772	3.611405	0.002909	0.282987
-10.100561	-2.033614	3.621402	0.002828	0.283235
-9.795591	-2.047229	3.631398	0.002771	0.283448
-9.692521	-2.025195	3.641395	0.002752	0.283656
-9.722387	-1.969363	3.651392	0.002758	0.283913
-9.955752	-1.863678	3.661389	0.002801	0.284235
-9.853182	-1.831714	3.671386	0.002782	0.284492
-9.804096	-1.781877	3.681382	0.002773	0.284790
-8.584739	-1.955687	3.691379	0.002546	0.285033
-8.498146	-1.925122	3.701376	0.002530	0.285268
-8.517477	-1.868467	3.711373	0.002534	0.285537
-7.455191	-2.015471	3.721370	0.002336	0.285770
-8.543925	-1.770952	3.731366	0.002539	0.286006
-7.956401	-1.819266	3.741363	0.002430	0.286301
-7.221020	-1.905439	3.751360	0.002293	0.286541
-6.782174	-1.939488	3.761357	0.002211	0.286771
-5.990204	-2.034276	3.771354	0.002064	0.287019
-6.251089	-1.939004	3.781350	0.002112	0.287260
-6.307379	-1.883519	3.791347	0.002123	0.287487
-6.432531	-1.806826	3.801344	0.002146	0.287758
-5.625900	-1.904635	3.811341	0.001996	0.288004
-6.180438	-1.746318	3.821338	0.002100	0.288292
-5.608762	-1.791532	3.831334	0.001993	0.288586
-5.398556	-1.780503	3.841331	0.001954	0.288833
-5.769937	-1.651154	3.851328	0.002023	0.289142
-5.136735	-1.713085	3.861325	0.001905	0.289408
-4.880880	-1.705203	3.871322	0.001858	0.289679
-4.189672	-1.782384	3.881318	0.001729	0.289921
-4.896891	-1.591992	3.891315	0.001861	0.290229
-4.923914	-1.519524	3.901312	0.001866	0.290565
-5.371348	-1.380737	3.911309	0.001949	0.290851
-4.199943	-1.531858	3.921306	0.001731	0.291158
-4.217060	-1.466042	3.931302	0.001735	0.291469
-3.187304	-1.596506	3.941299	0.001543	0.291750
-3.656203	-1.451033	3.951296	0.001630	0.292048
-3.446475	-1.424763	3.961293	0.001591	0.292367
-3.319681	-1.384220	3.971290	0.001568	0.292681
-4.156070	-1.158832	3.981286	0.001723	0.293043
-3.823617	-1.146599	3.991283	0.001662	0.293402
-3.154731	-1.198795	4.001280	0.001537	0.293743
-2.517831	-1.247405	4.011277	0.001419	0.294074
-1.965493	-1.284732	4.021274	0.001316	0.294383
-2.594844	-1.101516	4.031270	0.001433	0.294721
-2.326192	-1.081320	4.041267	0.001383	0.295060
-3.428053	-0.799815	4.051264	0.001588	0.295457
-2.796271	-0.839223	4.061261	0.001471	0.295826
-2.554120	-0.802047	4.071258	0.001426	0.296223
-1.787733	-0.865738	4.081254	0.001283	0.296591
-1.760948	-0.798821	4.091251	0.001278	0.296941
-1.709069	-0.735790	4.101248	0.001269	0.297294
-1.265340	-0.731312	4.111245	0.001186	0.297707
-1.026659	-0.692063	4.121242	0.001142	0.298108
-1.043507	-0.617711	4.131238	0.001145	0.298454
-0.774735	-0.588613	4.141235	0.001095	0.298831
-1.237635	-0.413684	4.151232	0.001181	0.299270
-1.193694	-0.335720	4.161229	0.001173	0.299685
-0.717913	-0.340587	4.171226	0.001084	0.300079
-0.941605	-0.201783	4.181222	0.001126	0.300551
-0.103665	-0.277403	4.191219	0.000970	0.300920
0.050697	-0.223986	4.201216	0.000941	0.301311
0.338908	-0.187095	4.211213	0.000888	0.301739
-0.040887	-0.028700	4.221210	0.000958	0.302167
0.176999	0.011458	4.231206	0.000918	0.302548
-0.057269	0.164613	4.241203	0.000961	0.303076
0.000000	0.233632	4.251200	0.000951	0.303455

0.427810	0.426581	4.256205	0.000871	0.304743
1.578373	0.764024	4.261210	0.000657	0.307327
1.927647	1.542659	4.266214	0.000591	0.311266
2.392278	2.585467	4.271219	0.000504	0.316463
3.386877	3.816844	4.276224	0.000318	0.322855
5.162760	5.206110	4.281229	-0.000013	0.330438
6.190143	7.039133	4.286234	-0.000206	0.339165
7.037627	9.213065	4.291238	-0.000365	0.348954
9.202603	11.464361	4.296243	-0.000770	0.359750
10.570537	14.184773	4.301248	-0.001026	0.371497
12.497054	17.143911	4.306253	-0.001387	0.384164
14.936137	20.362713	4.311258	-0.001843	0.397711
18.051256	23.818759	4.316262	-0.002425	0.412074
21.137574	27.662981	4.321267	-0.003002	0.427249
24.897331	31.743721	4.326272	-0.003705	0.443072
29.036400	36.153601	4.331277	-0.004478	0.459600
32.211395	41.129479	4.336282	-0.005073	0.476741
35.118817	46.513781	4.341286	-0.005618	0.494338
39.971330	51.940736	4.346291	-0.006525	0.512439
45.720833	57.583014	4.351296	-0.007599	0.530945
50.050200	63.866442	4.356301	-0.008409	0.549837
56.471575	70.136802	4.361306	-0.009609	0.569020
62.948816	76.776488	4.366310	-0.010819	0.588504
81.868825	81.588709	4.371315	-0.014345	0.608319
94.328092	88.043898	4.376320	-0.016669	0.628607
116.150337	93.287927	4.381325	-0.020736	0.649282
122.183739	101.776234	4.386330	-0.021865	0.670207
127.301884	110.655583	4.391334	-0.022824	0.690968
131.709145	119.884277	4.396339	-0.023650	0.711570
136.039290	129.300700	4.401344	-0.024463	0.731930
145.509571	138.003040	4.406349	-0.026232	0.752118
153.325000	147.194107	4.411354	-0.027693	0.772133
161.058021	156.561676	4.416358	-0.029139	0.791930
173.706632	165.203668	4.421363	-0.031499	0.811493
199.756503	171.835988	4.426368	-0.036354	0.831206
210.226660	181.461608	4.431373	-0.038310	0.850851
223.204224	190.783051	4.436378	-0.040732	0.870271
233.829646	200.603230	4.441382	-0.042717	0.889392
249.320139	209.685852	4.446387	-0.045607	0.908286
263.758460	219.058602	4.451392	-0.048302	0.926945
272.133207	229.545680	4.456397	-0.049868	0.945305
280.659496	239.947404	4.461402	-0.051462	0.963219
285.916584	250.847559	4.466406	-0.052448	0.980693
291.537624	261.581808	4.471411	-0.053502	0.997710
295.865168	272.355063	4.476416	-0.054315	1.014174
301.390878	282.788000	4.481421	-0.055350	1.030186
308.114772	292.883411	4.486426	-0.056609	1.045771
314.735486	302.921900	4.491430	-0.057848	1.061021
320.149350	313.072221	4.496435	-0.058863	1.075921
323.039469	323.501420	4.501440	-0.059408	1.090407
324.920100	333.926944	4.506445	-0.059765	1.104471
327.215518	344.101323	4.511450	-0.060199	1.118126
329.583309	354.107464	4.516454	-0.060646	1.131416
332.309194	363.914293	4.521459	-0.061160	1.144378
336.309147	373.402109	4.526464	-0.061911	1.157068
341.154308	382.621019	4.531469	-0.062819	1.169466
346.035483	391.805128	4.536474	-0.063734	1.181695
352.211896	400.684569	4.541478	-0.064890	1.193696
359.761825	409.327425	4.546483	-0.066301	1.205570
366.008327	418.204273	4.551488	-0.067470	1.217339
371.375555	427.195020	4.556493	-0.068475	1.228950
376.146603	436.234100	4.561498	-0.069369	1.240389
380.730395	445.217522	4.566502	-0.070229	1.251620
384.950185	454.224371	4.571507	-0.071020	1.262706
388.680959	463.238121	4.576512	-0.071721	1.273608
392.435777	472.163524	4.581517	-0.072426	1.284321
395.467143	481.174647	4.586522	-0.072996	1.294904
397.446277	490.246306	4.591526	-0.073370	1.305272
399.495299	499.328126	4.596531	-0.073758	1.315580
401.228890	508.231146	4.601536	-0.074086	1.325558
402.872757	517.102697	4.606541	-0.074398	1.335410
404.424916	525.918116	4.611546	-0.074693	1.345113
405.720340	534.708950	4.616550	-0.074940	1.354674
407.460035	543.357348	4.621555	-0.075269	1.364096
409.272489	551.966717	4.626560	-0.075612	1.373424
411.131277	560.549313	4.631565	-0.075964	1.382669
412.833351	569.130304	4.636570	-0.076286	1.391823
414.128355	577.681769	4.641574	-0.076533	1.400817
415.255407	586.268942	4.646579	-0.076748	1.409762
416.500961	594.771953	4.651584	-0.076986	1.418584
417.354363	603.316575	4.656589	-0.077150	1.427328
418.197202	611.832808	4.661594	-0.077313	1.435988
418.590823	620.370198	4.666598	-0.077392	1.444544
419.297130	628.845143	4.671603	-0.077529	1.453038
420.050014	637.253527	4.676608	-0.077674	1.461425
421.385064	645.561255	4.681613	-0.077928	1.469759
422.294923	653.948644	4.686618	-0.078103	1.478054
423.097806	662.278887	4.691622	-0.078258	1.486232
423.818605	670.662749	4.696627	-0.078398	1.494402
424.768270	678.957377	4.701632	-0.078580	1.502479
425.032257	687.376287	4.706637	-0.078634	1.510523
426.089278	695.627637	4.711642	-0.078836	1.518489
426.601004	703.961943	4.716646	-0.078937	1.526407
427.343803	712.272739	4.721651	-0.079081	1.534298
427.932376	720.560255	4.726656	-0.079196	1.542103
428.659841	728.835761	4.731661	-0.079337	1.549878
429.415573	737.104384	4.736666	-0.079483	1.557612
429.515728	745.429880	4.741670	-0.079507	1.565262
430.376594	753.660851	4.746675	-0.079672	1.572901
430.892656	761.916738	4.751680	-0.079774	1.580475
431.429984	770.181777	4.756685	-0.079879	1.588023
431.919197	778.443972	4.761690	-0.079976	1.595527
432.260615	786.693618	4.766694	-0.080044	1.602963
433.134248	794.870046	4.771699	-0.080212	1.610375
433.729168	803.087934	4.776704	-0.080329	1.617750
434.292437	811.306963	4.781709	-0.080439	1.625087
435.106817	819.548399	4.786714	-0.080596	1.632447
435.583627	827.753764	4.791718	-0.080690	1.639694
436.715761	835.862170	4.796723	-0.080906	1.646917
437.250723	844.107162	4.801728	-0.081011	1.654143
437.962461	852.280469	4.806733	-0.081149	1.661299
438.426265	860.533814	4.811738	-0.081240	1.668460
439.942809	868.559376	4.816742	-0.081528	1.675538
441.158819	876.693349	4.821747	-0.081760	1.682638
441.866686	884.902053	4.826752	-0.081897	1.689703
442.242932	893.186343	4.831757	-0.081972	1.696757
443.028854	901.362441	4.836762	-0.082124	1.703745
443.089166	909.664143	4.841766	-0.082140	1.710714
444.043712	917.799342	4.846771	-0.082323	1.717634
444.913918	925.914329	4.851776	-0.082491	1.724497
445.473896	934.122859	4.856781	-0.082600	1.731370
445.885038	942.354815	4.861786	-0.082682	1.738215
446.230924	950.548276	4.866790	-0.082752	1.744994
446.989458	958.720082	4.871795	-0.082898	1.751782
447.988492	966.809303	4.876800	-0.083089	1.758506
448.237581	975.031084	4.881805	-0.083141	1.765217
449.287413	983.135591	4.886810	-0.083342	1.771908
450.153846	991.258095	4.891814	-0.083508	1.778566
450.821615	999.441272	4.896819	-0.083638	1.785222
451.061657	1007.717642	4.901824	-0.083688	1.791875
451.669651	1015.868108	4.906829	-0.083807	1.798448
452.706353	1023.943998	4.911834	-0.084005	1.804991
453.344141	1032.107415	4.916838	-0.084129	1.811530
454.110008	1040.257385	4.921843	-0.084277	1.818050
455.050039	1048.340442	4.926848	-0.084457	1.824515
455.631839	1056.542075	4.931853	-0.084571	1.831007
456.936123	1064.582597	4.936858	-0.084819	1.837437
457.682079	1072.717672	4.941862	-0.084963	1.843850
458.388193	1080.903464	4.946867	-0.085100	1.850276
459.760121	1088.951689	4.951872	-0.085360	1.856652
460.798381	1097.076330	4.956877	-0.085559	1.863025
462.043473	1105.194686	4.961882	-0.085796	1.869396
462.884111	1113.329412	4.966886	-0.085958	1.875709
464.177252	1121.417570	4.971891	-0.086204	1.882019
465.549036	1129.491818	4.976896	-0.086464	1.888305
466.482560	1137.660312	4.981901	-0.086644	1.894591
467.806773	1145.763021	4.986906	-0.086895	1.900851
468.182843	1154.007990	4.991910	-0.086971	1.907089
468.397020	1162.279176	4.996915	-0.087016	1.913308
470.182557	1170.225325	5.001920	-0.087354	1.919441
472.171549	1178.187081	5.006925	-0.087729	1.925589
473.944165	1186.262278	5.011930	-0.088064	1.931777
476.076776	1194.268834	5.016934	-0.088467	1.937933
479.722547	1202.111927	5.021939	-0.089151	1.944117
482.442639	1210.145613	5.026944	-0.089662	1.950318
485.222829	1218.164980	5.031949	-0.090185	1.956494
487.682283	1226.263688	5.036954	-0.090648	1.962673
489.556442	1234.428946	5.041958	-0.091003	1.968817
490.658760	1242.710025	5.046963	-0.091213	1.974941
491.902744	1250.935441	5.051968	-0.091450	1.981021
492.946269	1259.157887	5.056973	-0.091650	1.987058
493.912717	1267.380745	5.061978	-0.091835	1.993069
494.431061	1275.620593	5.066982	-0.091937	1.999026
495.323836	1283.784356	5.071987	-0.092108	2.004950
496.532481	1291.911718	5.076992	-0.092339	2.010865
496.964636	1300.150829	5.081997	-0.092424	2.016759
497.653681	1308.317913	5.087002	-0.092558	2.022612
499.492377	1316.256202	5.092006	-0.092906	2.028406
500.157929	1324.473913	5.097011	-0.093035	2.034258
500.975605	1332.582065	5.102016	-0.093192	2.040031
501.637610	1340.720237	5.107021	-0.093321	2.045794
502.358396	1348.875748	5.112026	-0.093460	2.051558
503.047641	1356.985733	5.117030	-0.093594	2.057270
503.822971	1365.096541	5.122035	-0.093743	2.062977
504.223860	1373.271435	5.127040	-0.093823	2.068673
504.465739	1381.442361	5.132045	-0.093874	2.074335
504.438577	1389.653487	5.137050	-0.093874	2.079982
505.516870	1397.613147	5.142054	-0.094080	2.085552
506.489257	1405.681162	5.147059	-0.094266	2.091171
506.584987	1413.886185	5.152064	-0.094289	2.096780
507.541350	1421.906449	5.157069	-0.094473	2.102334
507.879888	1430.081015	5.162074	-0.094541	2.107917
508.630462	1438.138977	5.167078	-0.094686	2.113447
509.089775	1446.253546	5.172083	-0.094777	2.118971
509.776393	1454.290737	5.177088	-0.094910	2.124452
509.808076	1462.501051	5.182093	-0.094921	2.129970
510.277000	1470.609146	5.187098	-0.095013	2.135449
511.119565	1478.597290	5.192102	-0.095176	2.140868
511.436562	1486.728633	5.197107	-0.095240	2.146319
511.994463	1494.819593	5.202112	-0.095349	2.151753
512.308957	1502.932573	5.207117	-0.095413	2.157163
512.761044	1511.015806	5.212122	-0.095502	2.162554
513.096550	1519.113464	5.217126	-0.095570	2.167930
513.810543	1527.173759	5.222131	-0.095708	2.173303
514.423015	1535.242342	5.227136	-0.095827	2.178658
514.928118	1543.313344	5.232141	-0.095927	2.183992
515.130414	1551.475897	5.237146	-0.095969	2.189345
515.200749	1559.616150	5.242150	-0.095988	2.194658
515.438169	1567.713618	5.247155	-0.096037	2.199945
515.941847	1575.742541	5.252160	-0.096136	2.205200
516.576898	1583.797335	5.257165	-0.096260	2.210470
516.579151	1591.957852	5.262170	-0.096265	2.215739
517.646912	1599.887426	5.267174	-0.096469	2.220943
518.256305	1607.967436	5.272179	-0.096588	2.226190
518.348855	1616.137780	5.277184	-0.096611	2.231436
518.662092	1624.220755	5.282189	-0.096674	2.236633
519.243475	1632.279374	5.287194	-0.096788	2.241827
519.649391	1640.350451	5.292198	-0.096868	2.247000
519.725800	1648.506586	5.297203	-0.096888	2.252187
520.160711	1656.571957	5.302208	-0.096974	2.257336
520.669602	1664.608445	5.307213	-0.097074	2.262461
521.283384	1672.662090	5.312218	-0.097194	2.267595
521.764875	1680.772408	5.317222	-0.097288	2.272740
521.752637	1688.941486	5.322227	-0.097291	2.277868
521.977943	1696.997083	5.327232	-0.097339	2.282935
522.134591	1705.072728	5.332237	-0.097373	2.287996
522.716604	1713.101188	5.337242	-0.097487	2.293053
522.809928	1721.185224	5.342246	-0.097509	2.298092
523.038470	1729.259421	5.347251	-0.097557	2.303125
523.314690	1737.349443	5.352256	-0.097614	2.308161
524.234280	1745.307168	5.357261	-0.097790	2.313159
524.986450	1753.343425	5.362266	-0.097935	2.318180
524.822572	1761.483313	5.367270	-0.097910	2.323176
525.062878	1769.594842	5.372275	-0.097960	2.328179
525.450045	1777.663173	5.377280	-0.098037	2.333156
525.560838	1785.771059	5.382285	-0.098063	2.338124
525.787720	1793.855400	5.387290	-0.098111	2.343077
526.046368	1801.920881	5.392294	-0.098164	2.348010
527.165198	1809.870691	5.397299	-0.098377	2.352933
527.524295	1817.950053	5.402304	-0.098450	2.357862
528.101444	1825.975785	5.407309	-0.098562	2.362766
528.454786	1834.067433	5.412314	-0.098633	2.367682
529.064188	1842.099887	5.417318	-0.098752	2.372572
529.281671	1850.234822	5.422323	-0.098798	2.377482
529.412810	1858.353292	5.427328	-0.098827	2.382364
529.280326	1866.491020	5.432333	-0.098808	2.387228
530.114885	1874.446402	5.437338	-0.098968	2.392049
530.629003	1882.486425	5.442342	-0.099069	2.396886
531.159010	1890.507845	5.447347	-0.099173	2.401703
531.206070	1898.666184	5.452352	-0.099187	2.406554
531.699499	1906.719101	5.457357	-0.099284	2.411367
532.187268	1914.787351	5.462362	-0.099380	2.416179
533.022995	1922.768119	5.467366	-0.099541	2.420957
533.578905	1930.829367	5.472371	-0.099650	2.425752
534.060729	1938.949427	5.477376	-0.099745	2.430565
534.083778	1947.096527	5.482381	-0.099754	2.435349
534.386427	1955.165415	5.487386	-0.099816	2.440099
534.895676	1963.144698	5.492390	-0.099916	2.444804
535.622491	1971.164337	5.497395	-0.100057	2.449540
536.108107	1979.219070	5.502400	-0.100152	2.454268
535.940122	1987.379738	5.507405	-0.100126	2.458999
536.487590	1995.397638	5.512410	-0.100233	2.463693
536.590194	2003.510173	5.517414	-0.100258	2.468398
536.962473	2011.565456	5.522419	-0.100332	2.473082
537.377323	2019.599016	5.527424	-0.100415	2.477747
537.432021	2027.685676	5.532429	-0.100430	2.482408
537.956330	2035.718619	5.537434	-0.100533	2.487063
538.113863	2043.810773	5.542438	-0.100567	2.491717
538.806862	2051.821447	5.547443	-0.100702	2.496355
538.822826	2059.956992	5.552448	-0.100710	2.501005
539.159648	2067.993088	5.557453	-0.100778	2.505614
539.843295	2076.055695	5.562458	-0.100910	2.510254
540.530255	2084.040311	5.567462	-0.101043	2.514842
540.822694	2092.106965	5.572467	-0.101103	2.519440
541.806762	2100.071266	5.577472	-0.101291	2.524021
542.178458	2108.158523	5.582477	-0.101366	2.528618
542.458502	2116.263618	5.587482	-0.101423	2.533211
543.060828	2124.281907	5.592486	-0.101541	2.537769
543.426073	2132.356111	5.597491	-0.101614	2.542334
543.378814	2140.485680	5.602496	-0.101610	2.546892
543.670505	2148.556798	5.607501	-0.101670	2.551433
544.499994	2156.568267	5.612506	-0.101829	2.555971
545.005605	2164.568968	5.617510	-0.101929	2.560472
545.538975	2172.617850	5.622515	-0.102033	2.564994
546.204435	2180.681984	5.627520	-0.102162	2.569525
546.605169	2188.751429	5.632525	-0.102242	2.574033
546.952432	2196.843429	5.637530	-0.102312	2.578541
547.399703	2204.865482	5.642534	-0.102401	2.583010
548.186698	2212.877110	5.647539	-0.102552	2.587488
548.672097	2221.038466	5.652544	-0.102648	2.592021
548.708180	2229.159422	5.657549	-0.102660	2.596492
549.320576	2237.159729	5.662554	-0.102779	2.600929
549.945350	2245.111847	5.667558	-0.102901	2.605332
549.806721	2253.253785	5.672563	-0.102880	2.609780
550.614597	2261.227636	5.677568	-0.103036	2.614193
550.618145	2269.332641	5.682573	-0.103042	2.618615
550.778302	2277.438803	5.687578	-0.103077	2.623041
551.244188	2285.441854	5.692582	-0.103169	2.627424
551.826163	2293.451099	5.697587	-0.103282	2.631811
552.590910	2301.456675	5.702592	-0.103430	2.636200
552.453425	2309.586194	5.707597	-0.103409	2.640589
553.053407	2317.600452	5.712602	-0.103526	2.644957
553.103012	2325.675427	5.717606	-0.103541	2.649315
553.461131	2333.734568	5.722611	-0.103613	2.653677
553.992396	2341.770855	5.727616	-0.103717	2.658031
555.022222	2349.670539	5.732621	-0.103914	2.662337
555.791532	2357.735034	5.737626	-0.104062	2.666707
555.959040	2365.851569	5.742630	-0.104098	2.671059
556.068875	2373.963891	5.747635	-0.104124	2.675397
556.337597	2382.010349	5.752640	-0.104179	2.679704
556.263445	2390.099205	5.757645	-0.104171	2.684003
556.987119	2398.103141	5.762650	-0.104311	2.688303
557.200331	2406.170889	5.767654	-0.104356	2.692596
557.381864	2414.247806	5.772659	-0.104395	2.696885
558.366480	2422.190035	5.777664	-0.104583	2.701148
558.768373	2430.242774	5.782669	-0.104663	2.705425
559.057238	2438.342830	5.787674	-0.104722	2.709713
559.249452	2446.406933	5.792678	-0.104763	2.713968
560.023748	2454.378996	5.797683	-0.104913	2.718206
559.919089	2462.531024	5.802688	-0.104898	2.722476
560.150540	2470.537554	5.807693	-0.104947	2.726684
561.021535	2478.561605	5.812698	-0.105114	2.730935
561.782558	2486.553718	5.817702	-0.105261	2.735155
561.687116	2494.692146	5.822707	-0.105248	2.739392
561.777852	2502.767022	5.827712	-0.105270	2.743601
562.247599	2510.774607	5.832717	-0.105363	2.747791
562.857697	2518.832891	5.837722	-0.105482	2.752010
563.246420	2526.890833	5.842726	-0.105559	2.756209
563.628031	2534.899926	5.847731	-0.105636	2.760376
564.028723	2542.921520	5.852736	-0.105716	2.764544
564.152217	2550.993462	5.857741	-0.105744	2.768714
564.542507	2559.037880	5.862746	-0.105822	2.772881
564.896169	2567.083118	5.867750	-0.105893	2.777039
564.781021	2575.192968	5.872755	-0.105876	2.781196
565.688469	2583.131616	5.877760	-0.106051	2.785320
566.014321	2591.188123	5.882765	-0.106116	2.789463
566.081727	2599.311909	5.887770	-0.106134	2.793620
566.147992	2607.357373	5.892774	-0.106152	2.797730
566.659736	2615.342253	5.897779	-0.106252	2.801829
567.053452	2623.395752	5.902784	-0.106331	2.805951
567.122853	2631.473562	5.907789	-0.106349	2.810059
567.295879	2639.540828	5.912794	-0.106386	2.814163
567.792793	2647.556182	5.917798	-0.106484	2.818252
567.989734	2655.601871	5.922803	-0.106526	2.822334
568.240245	2663.671735	5.927808	-0.106578	2.826425
568.529269	2671.696384	5.932813	-0.106637	2.830490
568.746237	2679.753997	5.937818	-0.106682	2.834561
568.889165	2687.782700	5.942822	-0.106714	2.838607
569.182261	2695.811439	5.947827	-0.106774	2.842656
569.880050	2703.800797	5.952832	-0.106909	2.846703
569.848902	2711.893393	5.957837	-0.106909	2.850754
570.066300	2719.948087	5.962842	-0.106954	2.854795
571.305373	2727.824930	5.967846	-0.107190	2.858798
571.636208	2735.895003	5.972851	-0.107257	2.862841
571.569462	2744.038430	5.977856	-0.107250	2.866893
572.213874	2752.023481	5.982861	-0.107375	2.870900
572.652919	2760.090305	5.987866	-0.107462	2.874930
572.721458	2768.144719	5.992870	-0.107480	2.878928
573.339787	2776.126751	5.997875	-0.107600	2.882914
573.894123	2784.173450	6.002880	-0.107708	2.886924
573.520336	2792.330743	6.007885	-0.107644	2.890931
574.074121	2800.340125	6.012890	-0.107752	2.894911
574.214155	2808.402385	6.017894	-0.107784	2.898889
574.515764	2816.424204	6.022899	-0.107845	2.902850
574.928748	2824.481715	6.027904	-0.107927	2.906830
575.588507	2832.483083	6.032909	-0.108055	2.910789
576.169363	2840.542697	6.037914	-0.108169	2.914768
576.183103	2848.594993	6.042918	-0.108176	2.918706
576.746223	2856.542114	6.047923	-0.108286	2.922618
577.396910	2864.545667	6.052928	-0.108413	2.926556
577.231864	2872.690153	6.057933	-0.108387	2.930514
577.128495	2880.788082	6.062938	-0.108373	2.934448
577.743153	2888.756049	6.067942	-0.108493	2.938351
578.106556	2896.772635	6.072947	-0.108566	2.942259
578.024287	2904.875006	6.077952	-0.108556	2.946180
578.505490	2912.828150	6.082957	-0.108650	2.950053
579.054957	2920.888709	6.087962	-0.108758	2.953976
578.990231	2928.963942	6.092966	-0.108751	2.957870
579.081523	2937.014784	6.097971	-0.108773	2.961754
579.738089	2945.000379	6.102976	-0.108901	2.965631
580.085777	2953.015721	6.107981	-0.108971	2.969502
579.978850	2961.141964	6.112986	-0.108956	2.973397
580.813367	2969.079464	6.117990	-0.109116	2.977244
581.100762	2977.150188	6.122995	-0.109175	2.981123
581.356017	2985.167062	6.128000	-0.109228	2.984969
581.340614	2993.282161	6.133005	-0.109230	2.988843
581.962223	3001.315096	6.138010	-0.109351	2.992705
581.916370	3009.372585	6.143014	-0.109348	2.996540
582.197033	3017.390649	6.148019	-0.109405	3.000368
582.577489	3025.385528	6.153024	-0.109481	3.004185
582.542613	3033.435321	6.158029	-0.109480	3.008002
582.921620	3041.499812	6.163034	-0.109556	3.011842
582.846113	3049.586335	6.168038	-0.109547	3.015665
583.149524	3057.557348	6.173043	-0.109609	3.019448
584.139470	3065.473807	6.178048	-0.109798	3.023233
584.713675	3073.502545	6.183053	-0.109910	3.027047
584.582195	3081.697716	6.188058	-0.109891	3.030899
584.826588	3089.719226	6.193062	-0.109942	3.034682
585.031798	3097.723032	6.198067	-0.109985	3.038451
585.320420	3105.787499	6.203072	-0.110044	3.042248
585.791801	3113.762560	6.208077	-0.110137	3.046007
586.396181	3121.762671	6.213082	-0.110255	3.049779
586.587218	3129.833754	6.218086	-0.110295	3.053560
586.814033	3137.892517	6.223091	-0.110343	3.057332
587.254914	3145.928608	6.228096	-0.110430	3.061099
587.007022	3154.015377	6.233101	-0.110389	3.064852
587.932184	3161.982957	6.238106	-0.110567	3.068601
588.059298	3170.083448	6.243110	-0.110596	3.072369
588.832924	3178.067326	6.248115	-0.110745	3.076109
589.106818	3186.118326	6.253120	-0.110801	3.079851
589.258678	3194.109989	6.258125	-0.110834	3.083556
589.635713	3202.168926	6.263130	-0.110910	3.087298
590.000955	3210.199108	6.268134	-0.110983	3.091022
590.369018	3218.216522	6.273139	-0.111057	3.094735
590.559739	3226.288120	6.278144	-0.111098	3.098461
590.664452	3234.306881	6.283149	-0.111122	3.102153
591.611378	3242.283903	6.288154	-0.111304	3.105861
591.832394	3250.322685	6.293158	-0.111350	3.109560
592.510278	3258.325403	6.298163	-0.111481	3.113258
592.734453	3266.419514	6.303168	-0.111528	3.116973
593.168270	3274.423224	6.308173	-0.111614	3.120651
592.810963	3282.542733	6.313178	-0.111553	3.124343
593.239450	3290.557289	6.318182	-0.111638	3.128017
593.415127	3298.630567	6.323187	-0.111676	3.131703
593.993701	3306.638563	6.328192	-0.111789	3.135372
594.179889	3314.657880	6.333197	-0.111829	3.139025
595.153180	3322.602168	6.338202	-0.112015	3.142675
595.535125	3330.680513	6.343206	-0.112091	3.146354
595.685391	3338.738145	6.348211	-0.112125	3.150010
596.935079	3346.651226	6.353216	-0.112362	3.153644
596.703148	3354.773577	6.358221	-0.112325	3.157304
596.831111	3362.856275	6.363226	-0.112354	3.160957
597.565737	3370.770109	6.368230	-0.112496	3.164556
597.349336	3378.931470	6.373235	-0.112460	3.168221
597.669216	3386.987642	6.378240	-0.112525	3.171858
597.918447	3394.989134	6.383245	-0.112577	3.175463
598.349838	3402.982252	6.388250	-0.112662	3.179068
598.842023	3411.016444	6.393254	-0.112759	3.182690
599.201980	3419.029500	6.398259	-0.112831	3.186292
599.663839	3427.090233	6.403264	-0.112923	3.189916
599.888028	3435.135585	6.408269	-0.112970	3.193519
599.918135	3443.212200	6.413274	-0.112980	3.197123
600.229691	3451.251467	6.418278	-0.113044	3.200719
600.778647	3459.173461	6.423283	-0.113151	3.204268
601.133330	3467.226262	6.428288	-0.113222	3.207864
601.295512	3475.307944	6.433293	-0.113258	3.211460
601.680616	3483.336833	6.438298	-0.113334	3.215037
602.495045	3491.294840	6.443302	-0.113491	3.218598
602.623261	3499.335212	6.448307	-0.113520	3.222162
603.063182	3507.391275	6.453312	-0.113607	3.225742
603.241922	3515.457685	6.458317	-0.113646	3.229312
603.811632	3523.453304	6.463322	-0.113757	3.232862
604.440016	3531.451809	6.468326	-0.113879	3.236413
604.923582	3539.433180	6.473331	-0.113975	3.239945
605.240259	3547.506534	6.478336	-0.114039	3.243508
605.118015	3555.607642	6.483341	-0.114021	3.247061
605.741543	3563.616415	6.488346	-0.114143	3.250600
606.017683	3571.639268	6.493350	-0.114199	3.254126
606.512685	3579.647203	6.498355	-0.114297	3.257652
606.662448	3587.743718	6.503360	-0.114330	3.261198
607.074817	3595.677674	6.508365	-0.114412	3.264680
607.217069	3603.779670	6.513370	-0.114443	3.268221
608.094640	3611.736531	6.518374	-0.114612	3.271724
608.451165	3619.757101	6.523379	-0.114683	3.275230
608.816886	3627.799975	6.528384	-0.114757	3.278742
608.953993	3635.845117	6.533389	-0.114787	3.282242
609.274957	3643.905999	6.538394	-0.114852	3.285753
609.457108	3651.955804	6.543398	-0.114892	3.289250
610.104234	3659.973720	6.548403	-0.115017	3.292747
610.403158	3668.044140	6.553408	-0.115078	3.296249
610.827039	3676.012299	6.558413	-0.115162	3.299709
611.119895	3684.049999	6.563418	-0.115222	3.303190
611.394425	3692.098691	6.568422	-0.115278	3.306671
611.774167	3700.132828	6.573427	-0.115354	3.310146
612.660442	3708.102866	6.578432	-0.115524	3.313609
613.074702	3716.125110	6.583437	-0.115607	3.317073
613.429852	3724.179382	6.588442	-0.115678	3.320545
613.727503	3732.194189	6.593446	-0.115739	3.323993
613.831921	3740.267348	6.598451	-0.115763	3.327456
614.457818	3748.317606	6.603456	-0.115885	3.330926
614.812039	3756.323020	6.608461	-0.115956	3.334362
615.323277	3764.332598	6.613466	-0.116056	3.337802
615.887391	3772.340207	6.618470	-0.116167	3.341239
616.035969	3780.371390	6.623475	-0.116200	3.344668
616.780387	3788.406643	6.628480	-0.116343	3.348117
617.041400	3796.455134	6.633485	-0.116397	3.351550
617.101195	3804.522852	6.638490	-0.116414	3.354980
617.454654	3812.521191	6.643494	-0.116485	3.358388
618.064708	3820.532188	6.648499	-0.116603	3.361807
617.870958	3828.629022	6.653504	-0.116572	3.365230
617.932525	3836.654484	6.658509	-0.116589	3.368628
618.400623	3844.684246	6.663514	-0.116681	3.372039
618.440841	3852.761211	6.668518	-0.116694	3.375452
618.705761	3860.726493	6.673523	-0.116749	3.378822
619.964883	3868.638873	6.678528	-0.116988	3.382202
619.897840	3876.747434	6.683533	-0.116981	3.385613
620.235100	3884.763022	6.688538	-0.117049	3.388996
620.241412	3892.931504	6.693542	-0.117055	3.392429
621.013030	3900.875489	6.698547	-0.117204	3.395790
621.398621	3908.855013	6.703552	-0.117281	3.399150
621.881928	3916.835904	6.708557	-0.117376	3.402510
622.609316	3924.871638	6.713562	-0.117517	3.405899
623.070374	3932.891676	6.718566	-0.117608	3.409268
623.446714	3940.939655	6.723571	-0.117683	3.412642
624.008029	3949.013333	6.728576	-0.117793	3.416030
623.987336	3957.022969	6.733581	-0.117794	3.419368
624.498515	3965.034629	6.738586	-0.117895	3.422721
624.820506	3973.116584	6.743590	-0.117960	3.426094
625.677774	3981.065577	6.748595	-0.118125	3.429427
625.692387	3989.152957	6.753600	-0.118133	3.432785
625.473163	3997.267456	6.758605	-0.118097	3.436143
626.122064	4005.197371	6.763610	-0.118223	3.439451
626.935001	4013.162586	6.768614	-0.118380	3.442775
627.237616	4021.196342	6.773619	-0.118441	3.446108
628.481526	4029.158513	6.778624	-0.118678	3.449439
628.706069	4037.237336	6.783629	-0.118725	3.452781
629.302692	4045.253105	6.788634	-0.118841	3.456106
629.442586	4053.355429	6.793638	-0.118872	3.459448
630.043887	4061.307088	6.798643	-0.118990	3.462740
630.671896	4069.367788	6.803648	-0.119112	3.466075
630.793915	4077.397216	6.808653	-0.119140	3.469376
631.015632	4085.475112	6.813658	-0.119186	3.472698
631.126160	4093.584191	6.818662	-0.119212	3.476026
632.021007	4101.395463	6.823667	-0.119384	3.479254
632.061601	4109.544753	6.828672	-0.119396	3.482590
632.293270	4117.563743	6.833677	-0.119445	3.485875
632.617924	4125.588431	6.838682	-0.119510	3.489162
633.614999	4133.518931	6.843686	-0.119701	3.492430
633.414887	4141.696910	6.848691	-0.119669	3.495757
633.779505	4149.695700	6.853696	-0.119742	3.499025
634.036529	4157.701336	6.858701	-0.119795	3.502290
634.766965	4165.674613	6.863706	-0.119936	3.505554
634.932666	4173.768784	6.868710	-0.119973	3.508846
635.149211	4181.767374	6.873715	-0.120018	3.512098
635.495519	4189.832812	6.878720	-0.120088	3.515377
635.950933	4197.788768	6.883725	-0.120178	3.518613
636.445362	4205.825704	6.888730	-0.120275	3.521879
636.645831	4213.866616	6.893734	-0.120317	3.525135
636.718040	4221.920236	6.898739	-0.120336	3.528389
637.078178	4229.986453	6.903744	-0.120408	3.531654
637.130437	4237.976799	6.908749	-0.120423	3.534876
637.885495	4245.951347	6.913754	-0.120569	3.538110
637.704084	4254.100757	6.918758	-0.120541	3.541383
637.720168	4262.067074	6.923763	-0.120549	3.544585
638.387549	4270.061537	6.928768	-0.120678	3.547816
638.864625	4278.116054	6.933773	-0.120772	3.551061
639.171764	4286.174541	6.938778	-0.120835	3.554300
639.430223	4294.219208	6.943782	-0.120888	3.557530
639.971030	4302.179210	6.948787	-0.120994	3.560730
640.324000	4310.167631	6.953792	-0.121065	3.563934
640.166022	4318.238850	6.958797	-0.121040	3.567152
641.117103	4326.151481	6.963802	-0.121223	3.570337
641.474261	4334.230626	6.968806	-0.121294	3.573568
641.657010	4342.244600	6.973811	-0.121334	3.576765
642.144032	4350.286680	6.978816	-0.121429	3.579979
642.732317	4358.259665	6.983821	-0.121544	3.583166
643.077918	4366.332446	6.988826	-0.121614	3.586382
643.663155	4374.367647	6.993830	-0.121728	3.589588
643.662021	4382.418210	6.998835	-0.121733	3.592779
644.136409	4390.462012	7.003840	-0.121826	3.595979
644.285638	4398.441970	7.008845	-0.121859	3.599141
645.256902	4406.396686	7.013850	-0.122045	3.602314
645.464064	4414.471454	7.018854	-0.122089	3.605510
645.259180	4422.545802	7.023859	-0.122056	3.608691
645.964279	4430.557447	7.028864	-0.122193	3.611870
645.851511	4438.645827	7.033869	-0.122177	3.615053
646.568301	4446.580810	7.038874	-0.122316	3.618197
647.110539	4454.610834	7.043878	-0.122422	3.621370
646.924125	4462.647954	7.048883	-0.122392	3.624523
647.302273	4470.703146	7.053888	-0.122468	3.627696
647.390032	4478.745355	7.058893	-0.122489	3.630853
647.827054	4486.761382	7.063898	-0.122576	3.634006
648.216320	4494.739254	7.068902	-0.122654	3.637141
647.970924	4502.816296	7.073907	-0.122613	3.640294
648.461294	4510.770030	7.078912	-0.122710	3.643416
649.239106	4518.755692	7.083917	-0.122860	3.646556
649.553486	4526.781402	7.088922	-0.122923	3.649696
650.160899	4534.813220	7.093926	-0.123042	3.652844
650.284624	4542.894282	7.098931	-0.123070	3.655995
650.845674	4550.848908	7.103936	-0.123179	3.659106
651.635423	4558.867241	7.108941	-0.123332	3.662245
652.044112	4566.879364	7.113946	-0.123413	3.665368
652.836192	4574.935252	7.118950	-0.123566	3.668516
653.282968	4582.963811	7.123955	-0.123654	3.671642
653.994089	4590.961431	7.128960	-0.123792	3.674759
654.439489	4598.979208	7.133965	-0.123880	3.677875
654.166495	4607.171682	7.138970	-0.123834	3.681037
655.030784	4615.046116	7.143974	-0.124000	3.684103
655.406933	4623.118581	7.148979	-0.124075	3.687230
655.687347	4631.163157	7.153984	-0.124133	3.690341
656.318880	4639.115219	7.158989	-0.124256	3.693423
656.961215	4647.154586	7.163994	-0.124380	3.696535
657.077899	4655.211318	7.168998	-0.124407	3.699639
657.453887	4663.239969	7.174003	-0.124483	3.702736
657.535549	4671.317559	7.179008	-0.124503	3.705841
657.983420	4679.317843	7.184013	-0.124592	3.708924
658.134673	4687.393162	7.189018	-0.124625	3.712025
658.648910	4695.414255	7.194022	-0.124726	3.715111
659.020572	4703.361759	7.199027	-0.124800	3.718164
659.710737	4711.388479	7.204032	-0.124934	3.721252
659.600650	4719.369894	7.209037	-0.124919	3.724300
659.841094	4727.426911	7.214042	-0.124969	3.727383
660.329085	4735.431511	7.219046	-0.125065	3.730450
660.728724	4743.424800	7.224051	-0.125144	3.733508
661.085430	4751.483298	7.229056	-0.125216	3.736587
661.140853	4759.512724	7.234061	-0.125231	3.739645
661.695688	4767.491762	7.239066	-0.125340	3.742693
661.669883	4775.599578	7.244070	-0.125340	3.745774
661.905009	4783.589122	7.249075	-0.125389	3.748813
662.308813	4791.649617	7.254080	-0.125470	3.751881
662.329815	4799.678157	7.259085	-0.125479	3.754926
662.697258	4807.633152	7.264090	-0.125552	3.757948
663.362405	4815.652186	7.269094	-0.125681	3.760999
663.516373	4823.640240	7.274099	-0.125715	3.764023
663.370889	4831.794567	7.279104	-0.125693	3.767101
663.877036	4839.716983	7.284109	-0.125793	3.770104
663.845437	4847.833656	7.289114	-0.125792	3.773166
664.823951	4855.767715	7.294118	-0.125979	3.776179
665.409712	4863.683502	7.299123	-0.126094	3.779174
665.665826	4871.844067	7.304128	-0.126147	3.782251
666.133641	4879.790141	7.309133	-0.126239	3.785250
665.888600	4887.930276	7.314138	-0.126198	3.788303
666.563740	4895.938473	7.319142	-0.126329	3.791324
666.336770	4903.975678	7.324147	-0.126292	3.794334
666.830095	4911.983734	7.329152	-0.126389	3.797347
667.162147	4919.975432	7.334157	-0.126456	3.800348
667.856147	4927.894581	7.339162	-0.126591	3.803327
668.286204	4935.984499	7.344166	-0.126676	3.806361
668.358631	4944.005977	7.349171	-0.126695	3.809360
668.796090	4952.076831	7.354176	-0.126781	3.812383
669.305169	4960.059682	7.359181	-0.126881	3.815372
669.717723	4968.060510	7.364186	-0.126963	3.818363
669.644400	4976.211721	7.369190	-0.126955	3.821397
669.689871	4984.165293	7.374195	-0.126968	3.824358
670.347407	4992.188041	7.379200	-0.127096	3.827356
670.355042	5000.247984	7.384205	-0.127103	3.830350
670.577914	5008.235467	7.389210	-0.127149	3.833321
671.616243	5016.235763	7.394214	-0.127348	3.836311
671.826939	5024.154166	7.399219	-0.127392	3.839250
672.380581	5032.219515	7.404224	-0.127501	3.842249
672.487306	5040.232261	7.409229	-0.127526	3.845217
673.218336	5048.230481	7.414234	-0.127667	3.848190
673.577120	5056.354128	7.419238	-0.127739	3.851200
673.971300	5064.319910	7.424243	-0.127817	3.854149
674.121888	5072.420660	7.429248	-0.127851	3.857141
674.114425	5080.467919	7.434253	-0.127855	3.860107
674.326354	5088.438026	7.439258	-0.127899	3.863048
674.519732	5096.529023	7.444262	-0.127940	3.866030
674.772548	5104.464306	7.449267	-0.127993	3.868953
675.081078	5112.589615	7.454272	-0.128055	3.871946
675.169176	5120.669581	7.459277	-0.128077	3.874915
675.291717	5128.639870	7.464282	-0.128105	3.877842
676.081207	5136.567379	7.469286	-0.128257	3.880765
676.295718	5144.518570	7.474291	-0.128302	3.883682
676.854487	5152.540948	7.479296	-0.128411	3.886630
676.987049	5160.552350	7.484301	-0.128441	3.889564
677.424997	5168.603135	7.489306	-0.128528	3.892515
677.732818	5176.646619	7.494310	-0.128590	3.895459
677.904944	5184.626500	7.499315	-0.128628	3.898375
677.883533	5192.796476	7.504320	-0.128629	3.901354
678.148790	5200.725395	7.509325	-0.128684	3.904249
678.731308	5208.744055	7.514330	-0.128797	3.907180
678.716210	5216.831912	7.519334	-0.128800	3.910123
679.840810	5224.705186	7.524339	-0.129014	3.913007
680.033014	5232.816955	7.529344	-0.129055	3.915958
679.846047	5240.832327	7.534349	-0.129025	3.918865
680.159037	5248.865780	7.539354	-0.129089	3.921785
680.620701	5256.862435	7.544358	-0.129180	3.924693
680.662979	5264.934878	7.549363	-0.129193	3.927618
681.246522	5272.900471	7.554368	-0.129307	3.930512
681.999832	5280.865334	7.559373	-0.129452	3.933407
682.232275	5288.962868	7.564378	-0.129501	3.936337
682.539241	5296.965952	7.569382	-0.129563	3.939233
682.985078	5304.978510	7.574387	-0.129651	3.942133
683.386287	5312.987263	7.579392	-0.129731	3.945028
683.974293	5320.979816	7.584397	-0.129846	3.947919
684.513134	5329.022548	7.589402	-0.129952	3.950825
684.813732	5337.093574	7.594406	-0.130013	3.953734
685.021466	5345.079680	7.599411	-0.130057	3.956609
685.670686	5353.068405	7.604416	-0.130183	3.959491
685.875856	5361.113519	7.609421	-0.130226	3.962383
686.185561	5369.097738	7.614426	-0.130289	3.965253
686.646388	5377.153776	7.619430	-0.130380	3.968148
686.671977	5385.249002	7.624435	-0.130390	3.971049
686.547746	5393.289275	7.629440	-0.130372	3.973925
687.099902	5401.269944	7.634445	-0.130480	3.976789
686.979939	5409.288478	7.639450	-0.130463	3.979653
687.971727	5417.202539	7.644454	-0.130653	3.982497
687.734530	5425.257476	7.649459	-0.130614	3.985368
687.540213	5433.366908	7.654464	-0.130583	3.988257
688.416416	5441.340216	7.659469	-0.130751	3.991113
688.978031	5449.283362	7.664474	-0.130861	3.993951
689.581596	5457.306812	7.669478	-0.130978	3.996817
689.765908	5465.323092	7.674483	-0.131018	3.999670
690.268049	5473.356979	7.679488	-0.131116	4.002534
690.415313	5481.389291	7.684493	-0.131149	4.005388
690.391862	5489.468607	7.689498	-0.131150	4.008255
691.133712	5497.489128	7.694502	-0.131293	4.011111
691.011788	5505.544028	7.699507	-0.131276	4.013963
691.011845	5513.613254	7.704512	-0.131281	4.016821
691.805046	5521.513352	7.709517	-0.131434	4.019628
691.850135	5529.561223	7.714522	-0.131447	4.022475
691.924600	5537.599378	7.719526	-0.131466	4.025316
692.424260	5545.563479	7.724531	-0.131565	4.028136
692.573804	5553.708068	7.729536	-0.131598	4.031012
693.166811	5561.724024	7.734541	-0.131713	4.033847
694.172105	5569.611830	7.739546	-0.131906	4.036642
694.515064	5577.630890	7.744550	-0.131975	4.039470
694.628068	5585.676282	7.749555	-0.132001	4.042303
694.796569	5593.718773	7.754560	-0.132037	4.045133
695.160172	5601.738200	7.759565	-0.132110	4.047956
695.585225	5609.745652	7.764570	-0.132195	4.050773
695.975141	5617.777266	7.769574	-0.132272	4.053597
695.851544	5625.830927	7.774579	-0.132255	4.056418
696.105604	5633.844907	7.779584	-0.132307	4.059230
696.203824	5641.892466	7.784589	-0.132331	4.062049
696.887384	5649.770500	7.789594	-0.132463	4.064815
697.376345	5657.887348	7.794598	-0.132559	4.067660
697.299801	5665.910876	7.799603	-0.132550	4.070462
697.541534	5673.943878	7.804608	-0.132600	4.073269
697.325301	5682.027145	7.809613	-0.132565	4.076086
698.222742	5689.905953	7.814618	-0.132738	4.078846
697.973488	5698.022291	7.819622	-0.132696	4.081670
698.409547	5705.909428	7.824627	-0.132783	4.084422
698.820446	5714.008641	7.829632	-0.132865	4.087246
699.107273	5722.032332	7.834637	-0.132923	4.090039
698.962163	5730.094899	7.839642	-0.132901	4.092838
699.751930	5738.047882	7.844646	-0.133054	4.095610
699.784876	5746.092036	7.849651	-0.133065	4.098402
700.556331	5754.082296	7.854656	-0.133214	4.101183
700.731039	5762.058175	7.859661	-0.133251	4.103948
701.328487	5770.062898	7.864666	-0.133368	4.106728
701.702243	5778.130627	7.869670	-0.133443	4.109524
701.692296	5786.198791	7.874675	-0.133446	4.112314
701.911186	5794.231208	7.879680	-0.133492	4.115092
702.275662	5802.195815	7.884685	-0.133565	4.117847
702.237719	5810.223578	7.889690	-0.133563	4.120616
702.688432	5818.220350	7.894694	-0.133652	4.123380
702.706224	5826.267784	7.899699	-0.133661	4.126153
703.066513	5834.260816	7.904704	-0.133733	4.128910
702.883261	5842.367382	7.909709	-0.133704	4.131697
703.541504	5850.307787	7.914714	-0.133832	4.134436
704.178227	5858.319045	7.919718	-0.133955	4.137197
704.700953	5866.280035	7.924723	-0.134058	4.139938
705.057636	5874.345325	7.929728	-0.134130	4.142710
704.954154	5882.400783	7.934733	-0.134116	4.145472
705.137167	5890.414011	7.939738	-0.134155	4.148220
705.383357	5898.520672	7.944742	-0.134206	4.151000
705.630011	5906.464969	7.949747	-0.134257	4.153722
706.206669	5914.481550	7.954752	-0.134369	4.156471
706.515049	5922.439935	7.959757	-0.134432	4.159195
706.807060	5930.539553	7.964762	-0.134492	4.161965
707.070012	5938.557867	7.969766	-0.134546	4.164705
707.152863	5946.550210	7.974771	-0.134566	4.167432
707.126059	5954.629433	7.979776	-0.134567	4.170186
707.637225	5962.629779	7.984781	-0.134667	4.172918
707.920730	5970.644164	7.989786	-0.134725	4.175650
708.290810	5978.624309	7.994790	-0.134799	4.178369
708.485231	5986.671686	7.999795	-0.134840	4.181107
708.846292	5994.638951	8.004800	-0.134913	4.183818
708.677759	6002.746674	8.009805	-0.134887	4.186569
709.332654	6010.670783	8.014810	-0.135014	4.189266
710.092194	6018.757125	8.019814	-0.135160	4.192016
710.336087	6026.771742	8.024819	-0.135211	4.194735
710.900641	6034.758326	8.029824	-0.135321	4.197446
711.114589	6042.750417	8.034829	-0.135366	4.200153
711.434315	6050.775803	8.039834	-0.135431	4.202870
711.534440	6058.832843	8.044838	-0.135455	4.205595
712.300073	6066.765227	8.049843	-0.135603	4.208282
712.358844	6074.885971	8.054848	-0.135619	4.211024
712.575659	6082.867357	8.059853	-0.135664	4.213718
712.854718	6090.879830	8.064858	-0.135721	4.216422
713.242961	6098.880333	8.069862	-0.135799	4.219122
713.395305	6106.958210	8.074867	-0.135832	4.221843
713.790033	6114.887411	8.079872	-0.135911	4.224515
713.900907	6123.016985	8.084877	-0.135937	4.227249
714.028135	6130.965506	8.089882	-0.135966	4.229921
714.467683	6139.023353	8.094886	-0.136053	4.232631
714.946626	6146.963488	8.099891	-0.136147	4.235301
715.043712	6155.020528	8.104896	-0.136171	4.238004
715.458637	6163.047474	8.109901	-0.136253	4.240698
715.932115	6171.007157	8.114906	-0.136346	4.243369
716.504337	6179.063472	8.119910	-0.136458	4.246071
716.632588	6187.093864	8.124915	-0.136487	4.248758
716.760352	6195.113532	8.129920	-0.136516	4.251440
717.402884	6203.066914	8.134925	-0.136641	4.254103
717.352102	6211.140202	8.139930	-0.136637	4.256798
718.066375	6219.150713	8.144934	-0.136775	4.259478
718.461335	6227.133155	8.149939	-0.136853	4.262143
718.672279	6235.145442	8.154944	-0.136898	4.264815
719.029830	6243.217038	8.159949	-0.136970	4.267506
719.373822	6251.210729	8.164954	-0.137039	4.270169
720.035731	6259.241489	8.169958	-0.137167	4.272846
720.499863	6267.221706	8.174963	-0.137259	4.275502
720.692206	6275.248983	8.179968	-0.137300	4.278171
720.910953	6283.337119	8.184973	-0.137346	4.280857
721.045326	6291.295167	8.189978	-0.137376	4.283499
721.210805	6299.362893	8.194982	-0.137412	4.286175
721.607657	6307.313928	8.199987	-0.137491	4.288813
721.950140	6315.409095	8.204992	-0.137560	4.291496
722.324620	6323.374666	8.209997	-0.137635	4.294135
722.473378	6331.444383	8.215002	-0.137668	4.296805
722.863324	6339.482072	8.220006	-0.137746	4.299464
723.096939	6347.484280	8.225011	-0.137794	4.302109
723.233106	6355.483466	8.230016	-0.137825	4.304751
723.769834	6363.515879	8.235021	-0.137930	4.307405
724.141288	6371.552672	8.240026	-0.138005	4.310057
724.777644	6379.503958	8.245030	-0.138128	4.312682
724.900715	6387.532127	8.250035	-0.138156	4.315326
725.477698	6395.500641	8.255040	-0.138269	4.317953
725.813780	6403.523478	8.260045	-0.138337	4.320594
726.005798	6411.509046	8.265050	-0.138378	4.323220
726.312069	6419.575886	8.270054	-0.138440	4.325872
726.609877	6427.590914	8.275059	-0.138500	4.328505
727.112376	6435.582599	8.280064	-0.138599	4.331130
727.518753	6443.596704	8.285069	-0.138680	4.333760
727.703744	6451.643562	8.290074	-0.138720	4.336398
727.842879	6459.663013	8.295078	-0.138751	4.339025
728.393531	6467.684288	8.300083	-0.138858	4.341654
728.504337	6475.638833	8.305088	-0.138884	4.344256
728.519335	6483.825717	8.310093	-0.138892	4.346932
728.811856	6491.779539	8.315098	-0.138952	4.349532
729.262901	6499.845945	8.320102	-0.139041	4.352168
729.529555	6507.824521	8.325107	-0.139096	4.354773
729.602960	6515.896197	8.330112	-0.139115	4.357405
729.856780	6523.903996	8.335117	-0.139167	4.360016
730.027381	6531.870409	8.340122	-0.139204	4.362611
730.824908	6539.807233	8.345126	-0.139358	4.365199
730.885731	6547.880591	8.350131	-0.139374	4.367825
731.512549	6555.862417	8.355136	-0.139496	4.370424
731.963600	6563.912212	8.360141	-0.139585	4.373042
732.220825	6571.905271	8.365146	-0.139638	4.375638
732.416311	6579.977494	8.370150	-0.139680	4.378259
732.042328	6588.041096	8.375155	-0.139616	4.380871
732.448039	6596.020896	8.380160	-0.139696	4.383459
733.108629	6604.009648	8.385165	-0.139825	4.386051
733.413894	6612.004937	8.390170	-0.139887	4.388640
733.834579	6620.092817	8.395174	-0.139970	4.391259
733.863782	6628.113348	8.400179	-0.139981	4.393852
733.989643	6636.167892	8.405184	-0.140009	4.396455
734.254799	6644.155251	8.410189	-0.140064	4.399036
734.740728	6652.180450	8.415194	-0.140160	4.401629
735.265630	6660.163454	8.420198	-0.140263	4.404206
735.412583	6668.179884	8.425203	-0.140295	4.406791
735.949914	6676.189864	8.430208	-0.140400	4.409374
736.256982	6684.268622	8.435213	-0.140463	4.411976
736.640960	6692.245260	8.440218	-0.140539	4.414545
737.347728	6700.274069	8.445222	-0.140676	4.417130
737.290068	6708.291573	8.450227	-0.140671	4.419707
737.704173	6716.313306	8.455232	-0.140753	4.422285
737.637784	6724.369551	8.460237	-0.140746	4.424871
737.986190	6732.344461	8.465242	-0.140816	4.427431
738.182299	6740.388720	8.470246	-0.140857	4.430011
738.374220	6748.401755	8.475251	-0.140898	4.432579
738.237320	6756.438874	8.480256	-0.140878	4.435152
738.952170	6764.404144	8.485261	-0.141016	4.437705
739.328482	6772.370237	8.490266	-0.141092	4.440255
739.628912	6780.414403	8.495270	-0.141153	4.442827
739.690306	6788.429461	8.500275	-0.141169	4.445388
740.205855	6796.449942	8.505280	-0.141271	4.447952
740.478568	6804.494123	8.510285	-0.141326	4.450520
740.625294	6812.515328	8.515290	-0.141359	4.453079
740.804224	6820.557457	8.520294	-0.141398	4.455643
741.361510	6828.479932	8.525299	-0.141506	4.458169
741.480055	6836.558722	8.530304	-0.141534	4.460741
741.782563	6844.518285	8.535309	-0.141595	4.463275
742.328579	6852.516893	8.540314	-0.141702	4.465821
742.162326	6860.617134	8.545318	-0.141676	4.468394
741.952572	6868.660554	8.550323	-0.141642	4.470949
742.553948	6876.591025	8.555328	-0.141760	4.473468
742.987444	6884.626528	8.560333	-0.141845	4.476019
743.591818	6892.553622	8.565338	-0.141963	4.478535
744.342391	6900.626727	8.570343	-0.142108	4.481096
744.630315	6908.576563	8.575347	-0.142167	4.483615
744.684069	6916.663662	8.580352	-0.142182	4.486175
745.044688	6924.682182	8.585357	-0.142254	4.488713
745.396660	6932.731159	8.590362	-0.142325	4.491259
745.497536	6940.783368	8.595367	-0.142349	4.493804
745.383656	6948.830394	8.600371	-0.142333	4.496345
746.373495	6956.702320	8.605376	-0.142523	4.498832
746.761411	6964.811274	8.610381	-0.142600	4.501391
747.419797	6972.666006	8.615386	-0.142728	4.503870
747.829216	6980.799099	8.620391	-0.142809	4.506433
747.985356	6988.780518	8.625395	-0.142843	4.508947
748.209126	6996.900833	8.630400	-0.142890	4.511503
748.711846	7004.828957	8.635405	-0.142989	4.513999
748.807958	7012.895083	8.640410	-0.143012	4.516535
749.061197	7020.874104	8.645415	-0.143065	4.519042
749.348861	7028.868340	8.650419	-0.143123	4.521553
749.350722	7036.886194	8.655424	-0.143129	4.524069
749.658744	7044.991914	8.660429	-0.143191	4.526613
749.644075	7052.897404	8.665434	-0.143194	4.529091
749.996522	7060.990088	8.670439	-0.143265	4.531627
750.341443	7068.957856	8.675443	-0.143334	4.534123
750.497621	7077.048131	8.680448	-0.143368	4.536655
751.011916	7084.933073	8.685453	-0.143469	4.539123
751.664046	7092.973516	8.690458	-0.143596	4.541637
752.125679	7100.978826	8.695463	-0.143687	4.544139
752.118714	7109.063418	8.700467	-0.143691	4.546664
752.272588	7117.033545	8.705472	-0.143725	4.549151
752.743912	7125.144584	8.710477	-0.143818	4.551682
752.766266	7133.071289	8.715482	-0.143827	4.554153
753.252705	7141.115300	8.720487	-0.143923	4.556660
753.606295	7149.061271	8.725491	-0.143994	4.559135
754.148672	7157.156352	8.730496	-0.144100	4.561655
754.205996	7165.106625	8.735501	-0.144116	4.564128
754.531322	7173.163602	8.740506	-0.144182	4.566633
755.107320	7181.204052	8.745511	-0.144294	4.569132
754.957384	7189.267941	8.750515	-0.144271	4.571636
754.925677	7197.205979	8.755520	-0.144271	4.574099
755.657415	7205.241381	8.760525	-0.144412	4.576593
755.856392	7213.214639	8.765530	-0.144454	4.579065
756.314240	7221.313482	8.770535	-0.144545	4.581574
756.734475	7229.230496	8.775539	-0.144628	4.584026
757.247584	7237.244512	8.780544	-0.144729	4.586507
757.365954	7245.328619	8.785549	-0.144756	4.589008
757.414658	7253.331480	8.790554	-0.144770	4.591482
758.130837	7261.321204	8.795559	-0.144909	4.593951
758.280818	7269.415616	8.800563	-0.144942	4.596451
758.428605	7277.328338	8.805568	-0.144975	4.598893
758.935126	7285.443254	8.810573	-0.145074	4.601397
759.165678	7293.347377	8.815578	-0.145122	4.603834
759.586796	7301.461326	8.820583	-0.145206	4.606334
759.636821	7309.431091	8.825587	-0.145220	4.608789
759.849549	7317.502431	8.830592	-0.145265	4.611273
760.555919	7325.405460	8.835597	-0.145402	4.613705
760.345510	7333.516244	8.840602	-0.145368	4.616199
760.612626	7341.527690	8.845607	-0.145423	4.618661
760.733631	7349.592298	8.850611	-0.145450	4.621138
761.214667	7357.488493	8.855616	-0.145545	4.623561
761.283560	7365.606596	8.860621	-0.145563	4.626052
761.476826	7373.534699	8.865626	-0.145604	4.628483
761.984056	7381.596764	8.870631	-0.145704	4.630954
762.478530	7389.530796	8.875635	-0.145801	4.633384
762.853134	7397.595510	8.880640	-0.145876	4.635853
763.150137	7405.630878	8.885645	-0.145937	4.638312
763.237564	7413.633500	8.890650	-0.145958	4.640759
763.566037	7421.629625	8.895655	-0.146024	4.643203
764.089181	7429.650966	8.900659	-0.146127	4.645653
764.374683	7437.663919	8.905664	-0.146185	4.648099
764.806779	7445.784945	8.910669	-0.146271	4.650577
764.641708	7453.786988	8.915674	-0.146246	4.653018
765.107946	7461.764312	8.920679	-0.146338	4.655450
765.133748	7469.813279	8.925683	-0.146348	4.657902
765.174986	7477.793746	8.930688	-0.146360	4.660332
765.970836	7485.790314	8.935693	-0.146514	4.662765
766.856086	7493.723958	8.940698	-0.146684	4.665177
766.984319	7501.849096	8.945703	-0.146713	4.667648
767.467629	7509.828998	8.950707	-0.146808	4.670072
767.553230	7517.904057	8.955712	-0.146829	4.672524
767.611868	7526.002825	8.960717	-0.146845	4.674982
767.819240	7533.942927	8.965722	-0.146889	4.677391
767.751859	7541.968245	8.970727	-0.146882	4.679825
768.401188	7549.910720	8.975731	-0.147008	4.682231
768.658328	7557.913185	8.980736	-0.147061	4.684654
769.010272	7565.969937	8.985741	-0.147132	4.687093
769.592685	7573.929144	8.990746	-0.147245	4.689500
770.218270	7582.008581	8.995751	-0.147367	4.691943
770.585668	7589.961760	9.000755	-0.147440	4.694346
770.278083	7598.096832	9.005760	-0.147388	4.696804
770.923409	7606.030241	9.010765	-0.147514	4.699199
771.356184	7614.047239	9.015770	-0.147599	4.701617
771.496519	7621.978524	9.020775	-0.147631	4.704009
771.616727	7630.150969	9.025779	-0.147658	4.706473
772.072740	7638.085617	9.030784	-0.147748	4.708863
772.742210	7646.156731	9.035789	-0.147878	4.711292
772.844185	7654.104457	9.040794	-0.147902	4.713684
773.572695	7662.194073	9.045799	-0.148043	4.716116
773.990500	7670.146480	9.050803	-0.148126	4.718506
774.556535	7678.129254	9.055808	-0.148237	4.720904
774.835541	7686.186654	9.060813	-0.148294	4.723324
775.072927	7694.204253	9.065818	-0.148343	4.725730
775.114575	7702.291947	9.070823	-0.148356	4.728157
775.608966	7710.279640	9.075827	-0.148454	4.730551
775.596545	7718.321052	9.080832	-0.148456	4.732961
775.378055	7726.390675	9.085837	-0.148421	4.735380
775.645192	7734.351197	9.090842	-0.148476	4.737763
776.298958	7742.313387	9.095847	-0.148603	4.740144
776.676711	7750.316736	9.100851	-0.148678	4.742537
776.515577	7758.316668	9.105856	-0.148653	4.744929
776.728196	7766.434210	9.110861	-0.148698	4.747355
777.255559	7774.387879	9.115866	-0.148802	4.749728
777.198384	7782.476434	9.120871	-0.148796	4.752143
777.770525	7790.376138	9.125875	-0.148908	4.754499
777.946164	7798.490191	9.130880	-0.148946	4.756918
778.602714	7806.405465	9.135885	-0.149073	4.759275
778.537037	7814.497862	9.140890	-0.149066	4.761686
779.352636	7822.376142	9.145895	-0.149223	4.764029
779.370413	7830.472522	9.150899	-0.149232	4.766439
779.910473	7838.451321	9.155904	-0.149337	4.768810
779.865978	7846.569894	9.160909	-0.149334	4.771224
780.449355	7854.462995	9.165914	-0.149448	4.773567
780.313253	7862.586501	9.170919	-0.149428	4.775981
780.855731	7870.563004	9.175923	-0.149534	4.778347
781.550963	7878.594109	9.180928	-0.149669	4.780727
781.735684	7886.598432	9.185933	-0.149708	4.783100
782.041100	7894.550505	9.190938	-0.149770	4.785456
782.574221	7902.565629	9.195943	-0.149875	4.787828
782.799580	7910.680821	9.200947	-0.149922	4.790230
783.285602	7918.604463	9.205952	-0.150018	4.792573
783.196246	7926.710748	9.210957	-0.150006	4.794972
783.684902	7934.675292	9.215962	-0.150102	4.797324
784.320225	7942.652451	9.220967	-0.150226	4.799679
784.389944	7950.728917	9.225971	-0.150244	4.802064
784.682388	7958.644626	9.230976	-0.150304	4.804400
785.585251	7966.740906	9.235981	-0.150477	4.806785
785.681049	7974.701931	9.240986	-0.150500	4.809132
785.585957	7982.830203	9.245991	-0.150488	4.811529
786.802322	7990.129158	9.250995	-0.150719	4.813673
786.892535	7994.805359	9.256000	-0.150739	4.815050

786.925710	7997.439614	9.261005	-0.150746	4.815826
786.968634	7998.860190	9.266010	-0.150755	4.816244
787.255509	7999.339920	9.271015	-0.150809	4.816384
787.128079	8000.284899	9.276019	-0.150786	4.816662
787.469141	8000.268152	9.281024	-0.150849	4.816656
787.763865	8000.301561	9.286029	-0.150904	4.816664
787.813958	8000.272674	9.291034	-0.150913	4.816655
787.978122	8000.317755	9.296039	-0.150944	4.816668
788.186557	8000.319010	9.301043	-0.150983	4.816667
787.889533	8000.347068	9.306048	-0.150927	4.816677
788.350007	8000.330138	9.311053	-0.151013	4.816670
788.699286	8000.300799	9.316058	-0.151078	4.816660
788.674244	8000.316299	9.321063	-0.151073	4.816664
788.758039	8000.344169	9.326067	-0.151089	4.816672
788.928478	8000.347991	9.331072	-0.151121	4.816672
789.323333	8000.351211	9.336077	-0.151194	4.816671
789.429966	8000.306270	9.341082	-0.151214	4.816658
789.497476	8000.271301	9.346087	-0.151226	4.816647
789.225335	8000.285974	9.351091	-0.151176	4.816653
789.089631	8000.331496	9.356096	-0.151150	4.816667
789.179642	8000.379620	9.361101	-0.151167	4.816680
789.178978	8000.361575	9.366106	-0.151167	4.816675
789.708720	8000.329863	9.371111	-0.151266	4.816663
789.935734	8000.292179	9.376115	-0.151308	4.816651
789.776304	8000.335195	9.381120	-0.151278	4.816665
789.991156	8000.419286	9.386125	-0.151318	4.816688
790.291678	8000.353097	9.391130	-0.151374	4.816667
790.024177	8000.389056	9.396135	-0.151324	4.816679
789.798045	8000.402353	9.401139	-0.151282	4.816684
790.018379	8000.357136	9.406144	-0.151323	4.816670
790.379419	8000.366174	9.411149	-0.151390	4.816671
790.103253	8000.347901	9.416154	-0.151339	4.816667
790.281873	8000.364584	9.421159	-0.151372	4.816671
790.001734	8000.388671	9.426163	-0.151320	4.816679
790.441584	8000.395807	9.431168	-0.151402	4.816679
790.569404	8000.405303	9.436173	-0.151425	4.816681
790.741114	8000.345508	9.441178	-0.151457	4.816663
790.943363	8000.377426	9.446183	-0.151495	4.816671
791.087982	8000.362800	9.451187	-0.151522	4.816666
790.288134	8000.443148	9.456192	-0.151373	4.816694
791.098676	8000.424485	9.461197	-0.151524	4.816685
791.135378	8000.359316	9.466202	-0.151530	4.816665
790.960892	8000.422240	9.471207	-0.151498	4.816685
791.422847	8000.356552	9.476211	-0.151584	4.816663
791.441949	8000.334585	9.481216	-0.151587	4.816656
791.328322	8000.390012	9.486221	-0.151566	4.816673
791.493602	8000.370419	9.491226	-0.151597	4.816667
791.721149	8000.345472	9.496231	-0.151639	4.816658
791.329161	8000.364560	9.501235	-0.151566	4.816666
791.191122	8000.433379	9.506240	-0.151541	4.816687
791.175583	8000.458579	9.511245	-0.151538	4.816694
791.069924	8000.408069	9.516250	-0.151518	4.816680
791.087486	8000.436989	9.521255	-0.151521	4.816688
791.017098	8000.474026	9.526259	-0.151508	4.816700
791.422695	8000.402120	9.531264	-0.151583	4.816676
791.583891	8000.427008	9.536269	-0.151613	4.816683
791.577731	8000.391903	9.541274	-0.151612	4.816673
791.424078	8000.401071	9.546279	-0.151584	4.816676
791.565868	8000.386400	9.551283	-0.151610	4.816671
791.891894	8000.413965	9.556288	-0.151671	4.816678
792.163494	8000.437466	9.561293	-0.151721	4.816683
792.205506	8000.396778	9.566298	-0.151729	4.816671
792.412201	8000.401193	9.571303	-0.151767	4.816671
792.292731	8000.419402	9.576307	-0.151745	4.816677
792.578689	8000.382677	9.581312	-0.151798	4.816665
792.527369	8000.421085	9.586317	-0.151789	4.816677
792.245063	8000.435588	9.591322	-0.151736	4.816682
792.619854	8000.407731	9.596327	-0.151806	4.816672
792.761453	8000.402604	9.601331	-0.151832	4.816670
792.775840	8000.380559	9.606336	-0.151835	4.816664
792.842386	8000.381637	9.611341	-0.151847	4.816664
792.628060	8000.389819	9.616346	-0.151807	4.816667
792.683465	8000.415112	9.621351	-0.151818	4.816674
792.722735	8000.379682	9.626355	-0.151825	4.816664
792.813056	8000.354629	9.631360	-0.151842	4.816656
793.068590	8000.417116	9.636365	-0.151889	4.816673
792.725235	8000.433808	9.641370	-0.151825	4.816680
792.920306	8000.450764	9.646375	-0.151861	4.816684
793.131312	8000.436157	9.651379	-0.151901	4.816678
793.126594	8000.438198	9.656384	-0.151900	4.816679
793.117531	8000.409408	9.661389	-0.151898	4.816670
793.327301	8000.373568	9.666394	-0.151937	4.816659
792.859025	8000.422172	9.671399	-0.151850	4.816675
793.370587	8000.419875	9.676403	-0.151945	4.816672
793.539639	8000.370644	9.681408	-0.151976	4.816657
793.253098	8000.442355	9.686413	-0.151923	4.816680
793.371127	8000.419873	9.691418	-0.151945	4.816672
793.361864	8000.448358	9.696423	-0.151943	4.816681
793.261248	8000.454145	9.701427	-0.151924	4.816683
793.202510	8000.366208	9.706432	-0.151913	4.816657
793.164690	8000.484390	9.711437	-0.151906	4.816692
793.154081	8000.433300	9.716442	-0.151904	4.816677
793.026697	8000.496990	9.721447	-0.151881	4.816697
793.284789	8000.472542	9.726451	-0.151929	4.816688
792.815887	8000.505225	9.731456	-0.151841	4.816700
793.007583	8000.393780	9.736461	-0.151877	4.816666
793.036648	8000.504563	9.741466	-0.151882	4.816699
793.433059	8000.452663	9.746471	-0.151956	4.816682
792.963578	8000.516097	9.751475	-0.151869	4.816703
793.141501	8000.387457	9.756480	-0.151902	4.816664
793.575546	8000.481486	9.761485	-0.151983	4.816690
793.849770	8000.413811	9.766490	-0.152034	4.816668
793.870550	8000.421571	9.771495	-0.152037	4.816670
794.006375	8000.434383	9.776499	-0.152063	4.816674
794.039665	8000.400977	9.781504	-0.152069	4.816664
793.985407	8000.455249	9.786509	-0.152059	4.816680
794.157914	8000.421986	9.791514	-0.152091	4.816669
794.232405	8000.428497	9.796519	-0.152105	4.816671
793.522081	8000.484832	9.801523	-0.151972	4.816691
793.210011	8000.350350	9.806528	-0.151914	4.816653
793.502806	8000.441022	9.811533	-0.151969	4.816678
793.439730	8000.439994	9.816538	-0.151957	4.816678
793.921379	8000.451002	9.821543	-0.152046	4.816679
794.101608	8000.442260	9.826547	-0.152080	4.816675
793.761960	8000.447342	9.831552	-0.152017	4.816679
793.827788	8000.473866	9.836557	-0.152029	4.816686
793.676757	8000.467165	9.841562	-0.152001	4.816685
793.818833	8000.355973	9.846567	-0.152027	4.816651
794.018267	8000.473771	9.851571	-0.152064	4.816685
793.884473	8000.452499	9.856576	-0.152039	4.816680
794.596534	8000.441797	9.861581	-0.152172	4.816673
794.339728	8000.416403	9.866586	-0.152124	4.816667
795.019500	8000.409421	9.871591	-0.152250	4.816661
794.893435	8000.410550	9.876595	-0.152227	4.816662
794.786449	8000.424718	9.881600	-0.152207	4.816667
794.895524	8000.430731	9.886605	-0.152227	4.816668
794.028993	8000.505739	9.891610	-0.152066	4.816695
794.043003	8000.396708	9.896615	-0.152068	4.816662
794.540199	8000.427064	9.901619	-0.152161	4.816669
794.973419	8000.352427	9.906624	-0.152242	4.816645
795.150944	8000.427442	9.911629	-0.152275	4.816666
795.257967	8000.420694	9.916634	-0.152295	4.816664
794.610508	8000.450469	9.921639	-0.152174	4.816675
794.478325	8000.492867	9.926643	-0.152149	4.816689
794.837547	8000.422331	9.931648	-0.152216	4.816666
794.667219	8000.465170	9.936653	-0.152184	4.816680
794.653040	8000.445843	9.941658	-0.152182	4.816674
795.121797	8000.457706	9.946663	-0.152269	4.816675
795.077088	8000.448489	9.951667	-0.152261	4.816673
794.626477	8000.419942	9.956672	-0.152177	4.816666
794.883907	8000.390181	9.961677	-0.152225	4.816656
794.927334	8000.454529	9.966682	-0.152233	4.816675
794.905243	8000.420222	9.971687	-0.152228	4.816665
794.936820	8000.456798	9.976691	-0.152234	4.816676
795.484132	8000.390383	9.981696	-0.152336	4.816654
795.330352	8000.420761	9.986701	-0.152307	4.816663
795.279833	8000.364777	9.991706	-0.152298	4.816647
795.857102	8000.287180	9.996711	-0.152405	4.816621
795.434078	8000.416073	10.001715	-0.152327	4.816661
795.421743	8000.363892	10.006720	-0.152324	4.816646
795.639736	8000.373799	10.011725	-0.152365	4.816648
795.775295	8000.357968	10.016730	-0.152390	4.816643
795.577095	8000.354740	10.021735	-0.152353	4.816643
795.450568	8000.398291	10.026739	-0.152330	4.816656
795.683701	8000.349042	10.031744	-0.152373	4.816640
795.713071	8000.387704	10.036749	-0.152378	4.816652
795.368592	8000.395887	10.041754	-0.152314	4.816656
796.022709	8000.383187	10.046759	-0.152436	4.816649
795.699099	8000.417167	10.051763	-0.152376	4.816660
795.810185	8000.372297	10.056768	-0.152396	4.816647
796.018277	8000.396895	10.061773	-0.152435	4.816653
796.118756	8000.328515	10.066778	-0.152454	4.816632
796.174805	8000.364429	10.071783	-0.152464	4.816643
796.307105	8000.381429	10.076787	-0.152489	4.816647
796.174484	8000.264704	10.081792	-0.152464	4.816613
796.037730	8000.340973	10.086797	-0.152438	4.816636
796.083047	8000.314126	10.091802	-0.152447	4.816628
796.049496	8000.350704	10.096807	-0.152440	4.816639
796.256823	8000.339223	10.101811	-0.152479	4.816635
796.198117	8000.331899	10.106816	-0.152468	4.816633
796.181500	8000.380421	10.111821	-0.152465	4.816647
796.182692	8000.370890	10.116826	-0.152465	4.816645
796.313949	8000.311497	10.121831	-0.152489	4.816626
796.242357	8000.378219	10.126835	-0.152476	4.816646
796.033580	8000.342995	10.131840	-0.152437	4.816637
796.255350	8000.351904	10.136845	-0.152478	4.816639
796.244264	8000.377179	10.141850	-0.152476	4.816646
796.592159	8000.354195	10.146855	-0.152541	4.816638
796.466533	8000.409430	10.151859	-0.152518	4.816655
795.899078	8000.410800	10.156864	-0.152412	4.816658
795.772404	8000.436316	10.161869	-0.152388	4.816666
796.125033	8000.393254	10.166874	-0.152454	4.816651
796.009155	8000.403034	10.171879	-0.152432	4.816655
796.075992	8000.395632	10.176883	-0.152445	4.816652
795.987160	8000.387818	10.181888	-0.152428	4.816650
795.720802	8000.441824	10.186893	-0.152379	4.816668
795.381027	8000.438414	10.191898	-0.152315	4.816668
795.596844	8000.396309	10.196903	-0.152355	4.816655
795.874006	8000.447488	10.201907	-0.152407	4.816669
795.788886	8000.412155	10.206912	-0.152391	4.816659
796.345537	8000.416966	10.211917	-0.152495	4.816657
796.219752	8000.383092	10.216922	-0.152471	4.816648
795.670285	8000.454767	10.221927	-0.152369	4.816672
796.048504	8000.420608	10.226931	-0.152439	4.816660
796.007896	8000.392364	10.231936	-0.152432	4.816652
795.877893	8000.470864	10.236941	-0.152407	4.816675
796.090562	8000.385215	10.241946	-0.152447	4.816649
796.076352	8000.449688	10.246951	-0.152444	4.816668
795.861142	8000.411178	10.251955	-0.152404	4.816658
795.491046	8000.417882	10.256960	-0.152335	4.816662
795.150632	8000.432496	10.261965	-0.152272	4.816668
795.263437	8000.435388	10.266970	-0.152293	4.816668
795.579778	8000.460685	10.271975	-0.152352	4.816674
795.671914	8000.470667	10.276979	-0.152369	4.816676
795.683153	8000.419929	10.281984	-0.152371	4.816661
795.708158	8000.447913	10.286989	-0.152375	4.816670
795.640034	8000.332238	10.291994	-0.152363	4.816636
795.434327	8000.467849	10.296999	-0.152324	4.816677
795.756160	8000.450805	10.302003	-0.152384	4.816670
795.575194	8000.434067	10.307008	-0.152350	4.816666
795.730274	8000.454620	10.312013	-0.152379	4.816671
796.177510	8000.387638	10.317018	-0.152463	4.816650
796.218391	8000.445582	10.322023	-0.152470	4.816666
796.275094	8000.429529	10.327027	-0.152481	4.816661
796.198294	8000.427215	10.332032	-0.152466	4.816661
796.362666	8000.442616	10.337037	-0.152497	4.816665
796.315551	8000.432299	10.342042	-0.152488	4.816662
796.348748	8000.425410	10.347047	-0.152494	4.816660
796.708158	8000.405796	10.352051	-0.152561	4.816652
796.324111	8000.401664	10.357056	-0.152490	4.816653
796.658508	8000.432562	10.362061	-0.152552	4.816660
796.014308	8000.444352	10.367066	-0.152432	4.816667
795.768169	8000.470045	10.372071	-0.152386	4.816676
795.897344	8000.496541	10.377075	-0.152410	4.816683
796.298536	8000.366225	10.382080	-0.152485	4.816643
796.053200	8000.476794	10.387085	-0.152439	4.816676
796.278052	8000.458173	10.392090	-0.152481	4.816670
796.823440	8000.387486	10.397095	-0.152582	4.816646
796.727458	8000.446386	10.402099	-0.152564	4.816664
796.500288	8000.411922	10.407104	-0.152522	4.816655
796.581051	8000.422780	10.412109	-0.152537	4.816658
796.897000	8000.365332	10.417114	-0.152596	4.816640
796.539865	8000.411495	10.422119	-0.152529	4.816655
796.574129	8000.414170	10.427123	-0.152536	4.816655
796.454474	8000.380396	10.432128	-0.152513	4.816646
796.489655	8000.405363	10.437133	-0.152520	4.816653
796.456874	8000.431346	10.442138	-0.152514	4.816661
796.248309	8000.470380	10.447143	-0.152475	4.816674
796.545580	8000.449755	10.452147	-0.152530	4.816666
796.431836	8000.463813	10.457152	-0.152509	4.816671
796.462383	8000.465367	10.462157	-0.152514	4.816671
796.556580	8000.425526	10.467162	-0.152532	4.816659
796.505273	8000.415140	10.472167	-0.152522	4.816656
796.786184	8000.413343	10.477171	-0.152575	4.816654
796.323573	8000.445060	10.482176	-0.152488	4.816666
796.865138	8000.433716	10.487181	-0.152589	4.816660
796.202489	8000.386862	10.492186	-0.152466	4.816649
796.183807	8000.456566	10.497191	-0.152462	4.816670
796.042516	8000.496695	10.502195	-0.152436	4.816682
795.448301	8000.433984	10.507200	-0.152325	4.816667
795.550162	8000.404876	10.512205	-0.152344	4.816658
795.719491	8000.456422	10.517210	-0.152376	4.816672
796.345077	8000.496300	10.522215	-0.152492	4.816681
796.062437	8000.456691	10.527219	-0.152439	4.816670
795.613845	8000.360285	10.532224	-0.152356	4.816644
795.989836	8000.528697	10.537229	-0.152426	4.816692
795.434743	8000.306448	10.542234	-0.152322	4.816629
795.881984	8000.417675	10.547239	-0.152406	4.816660
795.812056	8000.293484	10.552243	-0.152393	4.816624
795.664105	8000.409880	10.557248	-0.152365	4.816659
795.508249	8000.239741	10.562253	-0.152336	4.816609
795.406931	8000.311282	10.567258	-0.152317	4.816631
795.320655	8000.291843	10.572263	-0.152301	4.816626
795.078938	7999.862554	10.577267	-0.152256	4.816500
795.013159	8000.124542	10.582272	-0.152243	4.816578
795.470728	8000.039693	10.587277	-0.152329	4.816551
795.221592	7999.993210	10.592282	-0.152282	4.816538
795.347364	8000.213764	10.597287	-0.152306	4.816602
795.321927	8000.027717	10.602291	-0.152301	4.816548
795.489740	8000.347606	10.607296	-0.152332	4.816641
795.768619	8000.372293	10.612301	-0.152384	4.816647
796.098216	8000.427509	10.617306	-0.152445	4.816662
796.074741	8000.429245	10.622311	-0.152441	4.816662
796.159067	8000.425309	10.627315	-0.152457	4.816661
796.141337	8000.417592	10.632320	-0.152453	4.816659
796.194567	8000.420576	10.637325	-0.152463	4.816659
796.194579	8000.373899	10.642330	-0.152463	4.816645
795.864208	8000.348365	10.647335	-0.152402	4.816640
795.855530	8000.059694	10.652339	-0.152400	4.816555
796.049979	8000.434121	10.657344	-0.152436	4.816664
796.080260	8000.392179	10.662349	-0.152442	4.816651
795.757522	8000.326461	10.667354	-0.152381	4.816634
795.752829	8000.381541	10.672359	-0.152381	4.816650
796.041106	8000.310913	10.677363	-0.152434	4.816628
795.612495	8000.359097	10.682368	-0.152354	4.816644
795.946221	8000.192678	10.687373	-0.152416	4.816593
795.953513	8000.326450	10.692378	-0.152418	4.816633
795.697861	8000.345624	10.697383	-0.152370	4.816640
795.713542	8000.043560	10.702387	-0.152373	4.816551
795.653970	8000.358693	10.707392	-0.152362	4.816644
795.156667	7999.838266	10.712397	-0.152269	4.816493
795.251819	7999.959671	10.717402	-0.152287	4.816528
795.476657	7999.989840	10.722407	-0.152329	4.816536
795.503314	7999.905411	10.727411	-0.152333	4.816511
795.503849	8000.098471	10.732416	-0.152334	4.816568
795.929511	8000.207222	10.737421	-0.152413	4.816598
795.757602	8000.207605	10.742426	-0.152381	4.816599
795.528786	7999.954605	10.747431	-0.152338	4.816525
795.636453	8000.078337	10.752435	-0.152358	4.816561
795.261263	8000.058444	10.757440	-0.152288	4.816557
795.482089	8000.052484	10.762445	-0.152329	4.816554
795.815520	8000.179889	10.767450	-0.152391	4.816590
795.967128	8000.354195	10.772455	-0.152420	4.816641
795.874871	8000.187212	10.777459	-0.152402	4.816592
795.598854	8000.126499	10.782464	-0.152351	4.816576
795.504592	7999.873568	10.787469	-0.152333	4.816502
795.980729	8000.291817	10.792474	-0.152422	4.816622
795.915542	8000.414863	10.797479	-0.152410	4.816659
795.864479	8000.304770	10.802483	-0.152400	4.816627
795.773816	8000.266165	10.807488	-0.152383	4.816616
796.355177	8000.351995	10.812493	-0.152492	4.816638
795.987876	8000.323739	10.817498	-0.152423	4.816632
796.570276	8000.516728	10.822503	-0.152532	4.816686
796.331905	8000.239163	10.827507	-0.152487	4.816605
796.086474	8000.407012	10.832512	-0.152441	4.816656
796.330560	8000.312328	10.837517	-0.152487	4.816627
796.004348	8000.206244	10.842522	-0.152426	4.816597
795.717522	7999.985183	10.847527	-0.152372	4.816533
796.085035	8000.240433	10.852531	-0.152441	4.816607
795.823571	8000.018722	10.857536	-0.152392	4.816543
796.363313	8000.243893	10.862541	-0.152493	4.816606
796.537163	8000.455692	10.867546	-0.152525	4.816668
796.267056	8000.173370	10.872551	-0.152475	4.816586
796.462846	8000.179733	10.877555	-0.152511	4.816587
796.567669	8000.472090	10.882560	-0.152531	4.816673
796.262410	8000.053417	10.887565	-0.152474	4.816551
796.116148	8000.061642	10.892570	-0.152446	4.816554
796.066120	8000.179631	10.897575	-0.152437	4.816589
796.357399	8000.389095	10.902579	-0.152491	4.816649
796.552202	8000.303156	10.907584	-0.152528	4.816623
796.196322	8000.230533	10.912589	-0.152461	4.816603
796.161367	8000.413475	10.917594	-0.152455	4.816657
795.762082	8000.196944	10.922599	-0.152380	4.816596
795.923133	7999.888760	10.927603	-0.152410	4.816504
796.111392	8000.265204	10.932608	-0.152445	4.816614
796.729319	8000.322989	10.937613	-0.152560	4.816628
797.056644	8000.488494	10.942618	-0.152621	4.816675
796.646866	8000.440449	10.947623	-0.152545	4.816663
796.905591	8000.444657	10.952627	-0.152593	4.816663
796.990836	8000.402548	10.957632	-0.152609	4.816650
797.216483	8000.531393	10.962637	-0.152651	4.816687
796.923118	8000.292177	10.967642	-0.152596	4.816618
797.068599	8000.435627	10.972647	-0.152623	4.816660
796.702660	8000.272670	10.977651	-0.152555	4.816613
796.587011	8000.186984	10.982656	-0.152533	4.816589
796.343259	8000.324098	10.987661	-0.152488	4.816630
796.766807	8000.288555	10.992666	-0.152567	4.816618
796.699061	8000.334124	10.997671	-0.152554	4.816631
796.716532	8000.448970	11.002675	-0.152557	4.816665
796.915069	8000.478718	11.007680	-0.152594	4.816673
797.114550	8000.403462	11.012685	-0.152631	4.816650
797.079063	8000.424097	11.017690	-0.152625	4.816656
796.795380	8000.427963	11.022695	-0.152572	4.816659
797.012926	8000.385886	11.027699	-0.152612	4.816645
797.185927	8000.480988	11.032704	-0.152645	4.816672
797.260985	8000.430227	11.037709	-0.152659	4.816657
797.164836	8000.522010	11.042714	-0.152641	4.816685
797.433534	8000.506226	11.047719	-0.152691	4.816679
797.293527	8000.433929	11.052723	-0.152664	4.816658
796.902841	8000.455147	11.057728	-0.152592	4.816666
797.476506	8000.359461	11.062733	-0.152698	4.816635
797.649699	8000.489576	11.067738	-0.152731	4.816673
797.265743	8000.429219	11.072743	-0.152659	4.816657
797.576389	8000.509591	11.077747	-0.152717	4.816679
797.565409	8000.459551	11.082752	-0.152715	4.816664
796.989460	8000.372732	11.087757	-0.152608	4.816641
797.601487	8000.499381	11.092762	-0.152722	4.816676
797.569039	8000.400193	11.097767	-0.152715	4.816647
797.442260	8000.530728	11.102771	-0.152692	4.816686
797.475456	8000.508988	11.107776	-0.152698	4.816679
797.620468	8000.381926	11.112781	-0.152725	4.816641
797.569707	8000.485056	11.117786	-0.152715	4.816672
797.527558	8000.463150	11.122791	-0.152708	4.816665
797.762996	8000.533812	11.127795	-0.152751	4.816685
797.765607	8000.433072	11.132800	-0.152752	4.816655
797.805627	8000.437964	11.137805	-0.152759	4.816657
797.344757	8000.376355	11.142810	-0.152673	4.816641
796.996675	8000.530867	11.147815	-0.152609	4.816688
797.597779	8000.425022	11.152819	-0.152720	4.816654
797.461082	8000.439766	11.157824	-0.152695	4.816659
797.749442	8000.525080	11.162829	-0.152749	4.816683
797.521135	8000.396182	11.167834	-0.152706	4.816646
797.605211	8000.418764	11.172839	-0.152722	4.816652
797.789208	8000.411148	11.177843	-0.152756	4.816649
797.726623	8000.479079	11.182848	-0.152744	4.816669
797.421802	8000.444409	11.187853	-0.152687	4.816660
797.593056	8000.439768	11.192858	-0.152719	4.816658
797.859843	8000.461082	11.197863	-0.152769	4.816663
797.531349	8000.527865	11.202867	-0.152708	4.816685
797.816943	8000.460376	11.207872	-0.152761	4.816663
797.610633	8000.424128	11.212877	-0.152722	4.816654
797.923551	8000.514086	11.217882	-0.152781	4.816679
797.799140	8000.491901	11.222887	-0.152757	4.816673
797.616854	8000.417854	11.227891	-0.152723	4.816652
797.424229	8000.498519	11.232896	-0.152687	4.816676
796.809689	8000.299689	11.237901	-0.152573	4.816621
797.332454	8000.375024	11.242906	-0.152670	4.816640
797.277079	8000.329565	11.247911	-0.152660	4.816627
797.739924	8000.518497	11.252915	-0.152746	4.816681
797.224142	8000.442203	11.257920	-0.152650	4.816661
797.409782	8000.459012	11.262925	-0.152684	4.816665
797.266564	8000.256185	11.267930	-0.152658	4.816606
797.490679	8000.388187	11.272935	-0.152699	4.816644
797.365968	8000.332052	11.277939	-0.152676	4.816628
797.472075	8000.362418	11.282944	-0.152696	4.816636
797.647141	8000.152042	11.287949	-0.152728	4.816573
797.663289	8000.225497	11.292954	-0.152731	4.816595
797.628391	8000.272661	11.297959	-0.152725	4.816609
798.002945	8000.342404	11.302963	-0.152795	4.816628
797.704519	8000.426651	11.307968	-0.152739	4.816654
797.814230	8000.460259	11.312973	-0.152759	4.816663
797.913583	8000.369581	11.317978	-0.152778	4.816636
797.925637	8000.430241	11.322983	-0.152780	4.816654
798.089467	8000.450939	11.327987	-0.152810	4.816659
797.379282	8000.377845	11.332992	-0.152678	4.816641
797.554476	8000.340383	11.337997	-0.152711	4.816629
797.450475	8000.444767	11.343002	-0.152691	4.816660
797.879997	8000.468731	11.348007	-0.152771	4.816665
798.183770	8000.476857	11.353011	-0.152828	4.816666
797.525237	8000.377021	11.358016	-0.152705	4.816640
797.917080	8000.402492	11.363021	-0.152778	4.816646
797.545998	8000.316886	11.368026	-0.152709	4.816622
797.789576	8000.397227	11.373031	-0.152754	4.816645
798.063426	8000.421838	11.378035	-0.152805	4.816651
798.107085	8000.509534	11.383040	-0.152813	4.816676
797.737682	8000.378337	11.388045	-0.152744	4.816640
797.983009	8000.378085	11.393050	-0.152790	4.816638
798.155216	8000.445596	11.398055	-0.152822	4.816657
798.385542	8000.509812	11.403059	-0.152865	4.816675
798.115871	8000.402515	11.408064	-0.152815	4.816645
798.031092	8000.419165	11.413069	-0.152799	4.816650
797.764189	8000.269484	11.418074	-0.152749	4.816607
797.736631	8000.375113	11.423079	-0.152744	4.816639
797.752876	8000.271414	11.428083	-0.152747	4.816608
798.066859	8000.446254	11.433088	-0.152805	4.816658
798.359659	8000.445715	11.438093	-0.152860	4.816656
798.670071	8000.458194	11.443098	-0.152918	4.816659
798.439372	8000.443824	11.448103	-0.152875	4.816655
798.233660	8000.281346	11.453107	-0.152836	4.816609
797.969504	8000.260068	11.458112	-0.152787	4.816604
798.486677	8000.436097	11.463117	-0.152883	4.816653
798.745960	8000.430769	11.468122	-0.152932	4.816650
798.956110	8000.451163	11.473127	-0.152971	4.816655
798.912809	8000.488645	11.478131	-0.152963	4.816666
799.267852	8000.459418	11.483136	-0.153029	4.816656
799.133337	8000.449796	11.488141	-0.153004	4.816654
799.141737	8000.476451	11.493146	-0.153005	4.816662
798.796165	8000.452783	11.498151	-0.152941	4.816656
798.850500	8000.514133	11.503155	-0.152951	4.816674
799.030559	8000.449169	11.508160	-0.152984	4.816654
798.818753	8000.500879	11.513165	-0.152945	4.816670
799.014861	8000.506192	11.518170	-0.152981	4.816671
798.954189	8000.446853	11.523175	-0.152970	4.816654
799.001643	8000.408371	11.528179	-0.152979	4.816642
799.367866	8000.433430	11.533184	-0.153047	4.816648
798.822344	8000.515772	11.538189	-0.152945	4.816675
798.713552	8000.432311	11.543194	-0.152925	4.816651
798.733143	8000.495216	11.548199	-0.152929	4.816669
798.530912	8000.461154	11.553203	-0.152891	4.816660
798.442880	8000.419405	11.558208	-0.152874	4.816648
798.384151	8000.523468	11.563213	-0.152864	4.816679
798.390919	8000.507662	11.568218	-0.152865	4.816675
798.224265	8000.428564	11.573223	-0.152834	4.816652
798.380838	8000.546742	11.578227	-0.152863	4.816686
798.251731	8000.443856	11.583232	-0.152839	4.816656
798.535997	8000.396501	11.588237	-0.152892	4.816641
798.730694	8000.400730	11.593242	-0.152928	4.816641
798.684856	8000.444535	11.598247	-0.152919	4.816655
798.630908	8000.470174	11.603251	-0.152909	4.816662
798.296905	8000.359707	11.608256	-0.152847	4.816631
798.627628	8000.392672	11.613261	-0.152908	4.816640
798.431270	8000.417052	11.618266	-0.152872	4.816648
798.644714	8000.334597	11.623271	-0.152911	4.816622
798.430309	8000.455219	11.628275	-0.152872	4.816659
798.451586	8000.305985	11.633280	-0.152875	4.816615
798.559234	8000.449887	11.638285	-0.152895	4.816657
798.640218	8000.427864	11.643290	-0.152911	4.816650
798.406885	8000.462250	11.648295	-0.152867	4.816661
798.810280	8000.435931	11.653299	-0.152942	4.816651
798.686681	8000.436036	11.658304	-0.152919	4.816652
798.633207	8000.401214	11.663309	-0.152909	4.816642
799.386351	8000.494106	11.668314	-0.153049	4.816666
799.434382	8000.440781	11.673319	-0.153058	4.816650
799.254775	8000.469676	11.678323	-0.153025	4.816659
798.867167	8000.405011	11.683328	-0.152952	4.816642
798.778408	8000.466152	11.688333	-0.152936	4.816660
798.660800	8000.311471	11.693338	-0.152914	4.816616
798.679586	8000.484691	11.698343	-0.152917	4.816666
798.966298	8000.247485	11.703347	-0.152971	4.816595
798.769205	8000.467049	11.708352	-0.152934	4.816661
798.797137	8000.467500	11.713357	-0.152939	4.816661
799.082091	8000.432887	11.718362	-0.152992	4.816649
799.211145	8000.509247	11.723367	-0.153016	4.816671
799.307306	8000.447158	11.728371	-0.153034	4.816652
799.111295	8000.447144	11.733376	-0.152998	4.816653
799.306149	8000.436524	11.738381	-0.153034	4.816649
799.013858	8000.429637	11.743386	-0.152979	4.816649
799.091333	8000.496668	11.748391	-0.152994	4.816668
799.471166	8000.510280	11.753395	-0.153064	4.816670
799.084299	8000.323628	11.758400	-0.152992	4.816617
799.053228	8000.459968	11.763405	-0.152986	4.816657
799.010131	8000.544131	11.768410	-0.152978	4.816682
798.826389	8000.452022	11.773415	-0.152944	4.816656
799.256790	8000.434631	11.778419	-0.153024	4.816649
798.836413	8000.360946	11.783424	-0.152946	4.816629
798.812698	8000.341461	11.788429	-0.152941	4.816624
798.833441	8000.344977	11.793434	-0.152945	4.816625
798.105813	8000.150664	11.798439	-0.152810	4.816571
798.475236	8000.339137	11.803443	-0.152878	4.816625
798.572004	8000.148699	11.808448	-0.152896	4.816568
798.578308	8000.310044	11.813453	-0.152898	4.816616
798.561564	8000.065778	11.818458	-0.152894	4.816544
798.617792	8000.349931	11.823463	-0.152905	4.816627
798.477910	8000.211863	11.828467	-0.152879	4.816587
798.242090	8000.148614	11.833472	-0.152835	4.816570
797.958218	7999.966836	11.838477	-0.152782	4.816517
798.773019	8000.228327	11.843482	-0.152934	4.816591
798.442363	8000.164594	11.848487	-0.152872	4.816573
798.739850	8000.217172	11.853491	-0.152927	4.816587
799.515309	8000.401657	11.858496	-0.153072	4.816638
799.291642	8000.533799	11.863501	-0.153030	4.816678
799.581957	8000.509883	11.868506	-0.153084	4.816670
799.442413	8000.424858	11.873511	-0.153058	4.816645
799.550849	8000.508309	11.878515	-0.153078	4.816669
799.306985	8000.512818	11.883520	-0.153033	4.816672
798.976377	8000.435290	11.888525	-0.152971	4.816650
799.336089	8000.494190	11.893530	-0.153038	4.816666
799.643995	8000.399482	11.898535	-0.153095	4.816637
799.285586	8000.510334	11.903539	-0.153029	4.816671
799.716330	8000.484463	11.908544	-0.153109	4.816661
799.211554	8000.527155	11.913549	-0.153015	4.816676
799.435142	8000.525491	11.918554	-0.153056	4.816675
799.528353	8000.423041	11.923559	-0.153074	4.816644
799.517512	8000.527887	11.928563	-0.153072	4.816675
799.520178	8000.516257	11.933568	-0.153072	4.816672
799.328398	8000.430381	11.938573	-0.153036	4.816647
799.557519	8000.509433	11.943578	-0.153079	4.816670
799.437405	8000.502167	11.948583	-0.153057	4.816668
799.414270	8000.451926	11.953587	-0.153052	4.816653
799.827082	8000.489415	11.958592	-0.153129	4.816662
799.464883	8000.500483	11.963597	-0.153062	4.816667
799.582382	8000.389942	11.968602	-0.153083	4.816634
799.739367	8000.420079	11.973607	-0.153113	4.816642
799.792353	8000.507931	11.978611	-0.153122	4.816668
799.632666	8000.504264	11.983616	-0.153093	4.816668
799.663444	8000.454901	11.988621	-0.153098	4.816653
799.824587	8000.494654	11.993626	-0.153128	4.816664
800.081126	8000.450032	11.998631	-0.153176	4.816650
800.008795	8000.488102	12.003635	-0.153162	4.816661
799.995340	8000.486818	12.008640	-0.153160	4.816661
800.055025	8000.486726	12.013645	-0.153171	4.816660
800.240515	8000.486564	12.018650	-0.153206	4.816660
800.535059	8000.481814	12.023655	-0.153260	4.816657
800.285962	8000.439558	12.028659	-0.153214	4.816645
799.973243	8000.505536	12.033664	-0.153156	4.816666
799.760369	8000.383245	12.038669	-0.153116	4.816631
799.902669	8000.402535	12.043674	-0.153142	4.816636
799.756106	8000.511534	12.048679	-0.153115	4.816669
799.681562	8000.448785	12.053683	-0.153101	4.816651
799.865508	8000.530285	12.058688	-0.153135	4.816674
800.022796	8000.519053	12.063693	-0.153165	4.816670
800.250957	8000.513221	12.068698	-0.153207	4.816667
799.768070	8000.439573	12.073703	-0.153117	4.816648
800.249386	8000.441048	12.078707	-0.153207	4.816646
799.714929	8000.326248	12.083712	-0.153107	4.816615
799.923271	8000.503622	12.088717	-0.153146	4.816666
800.445909	8000.450607	12.093722	-0.153243	4.816648
800.603131	8000.517881	12.098727	-0.153272	4.816667
799.915136	8000.467409	12.103731	-0.153144	4.816655
799.921400	8000.520552	12.108736	-0.153145	4.816671
800.141658	8000.422294	12.113741	-0.153186	4.816641
800.405771	8000.504040	12.118746	-0.153235	4.816664
800.216097	8000.505188	12.123751	-0.153200	4.816665
799.999299	8000.546208	12.128755	-0.153160	4.816678
799.717484	8000.330498	12.133760	-0.153107	4.816616
799.540998	8000.455983	12.138765	-0.153074	4.816654
800.209080	8000.525217	12.143770	-0.153199	4.816671
799.898670	8000.455440	12.148775	-0.153141	4.816652
799.531698	8000.258501	12.153779	-0.153072	4.816596
799.493319	8000.192100	12.158784	-0.153065	4.816576
800.037592	8000.395102	12.163789	-0.153167	4.816634
800.013222	8000.353327	12.168794	-0.153162	4.816621
800.144392	8000.513532	12.173799	-0.153186	4.816668
800.199209	8000.527153	12.178803	-0.153197	4.816672
800.250715	8000.438875	12.183808	-0.153206	4.816645
799.798368	8000.397551	12.188813	-0.153122	4.816635
799.977372	8000.394099	12.193818	-0.153155	4.816634
799.851341	8000.520408	12.198823	-0.153132	4.816671
799.748216	8000.359593	12.203827	-0.153112	4.816625
799.850807	8000.181975	12.208832	-0.153131	4.816572
799.447187	8000.171154	12.213837	-0.153056	4.816571
799.891181	8000.461634	12.218842	-0.153139	4.816654
799.832759	8000.447948	12.223847	-0.153128	4.816650
800.113407	8000.431301	12.228851	-0.153180	4.816644
799.698948	8000.268596	12.233856	-0.153103	4.816598
799.452436	8000.326106	12.238861	-0.153057	4.816616
799.324374	7999.849822	12.243866	-0.153033	4.816477
798.967463	8000.116640	12.248871	-0.152966	4.816557
798.769846	7999.797296	12.253875	-0.152929	4.816464
798.813975	8000.109890	12.258880	-0.152938	4.816556
799.507523	8000.253787	12.263885	-0.153067	4.816595
799.494767	8000.097631	12.268890	-0.153064	4.816549
799.073853	8000.087591	12.273895	-0.152986	4.816548
799.021494	7999.928672	12.278899	-0.152976	4.816501
799.057754	8000.019428	12.283904	-0.152983	4.816528
799.162406	8000.181315	12.288909	-0.153002	4.816575
800.034675	8000.431033	12.293914	-0.153165	4.816644
799.534564	8000.278602	12.298919	-0.153072	4.816602
799.571886	8000.036273	12.303923	-0.153078	4.816530
799.659569	8000.435518	12.308928	-0.153095	4.816647
799.717690	8000.448131	12.313933	-0.153106	4.816651
799.018303	7999.999667	12.318938	-0.152975	4.816522
799.155662	8000.277717	12.323943	-0.153001	4.816603
798.914963	8000.096634	12.328947	-0.152956	4.816551
799.148044	8000.047384	12.333952	-0.152999	4.816536
798.942817	7999.955991	12.338957	-0.152961	4.816510
798.696603	7999.838473	12.343962	-0.152915	4.816476
798.708779	7999.849276	12.348967	-0.152917	4.816479
798.660883	7999.897290	12.353971	-0.152908	4.816494
798.792682	7999.802898	12.358976	-0.152933	4.816465
799.137634	8000.141608	12.363981	-0.152997	4.816563
799.652603	8000.183939	12.368986	-0.153093	4.816573
799.700911	8000.530564	12.373991	-0.153102	4.816675
799.996131	8000.377301	12.378995	-0.153157	4.816629
799.696743	8000.466836	12.384000	-0.153101	4.816656
799.411102	8000.446265	12.389005	-0.153048	4.816652
799.895998	8000.248355	12.394010	-0.153138	4.816591
799.943923	8000.449637	12.399015	-0.153147	4.816650
799.754249	8000.330907	12.404019	-0.153112	4.816616
799.907924	8000.288852	12.409024	-0.153140	4.816603
799.725374	8000.245561	12.414029	-0.153106	4.816591
800.256908	8000.360306	12.419034	-0.153205	4.816622
800.093641	8000.391589	12.424039	-0.153175	4.816632
800.089143	8000.331043	12.429043	-0.153174	4.816615
800.265429	8000.400747	12.434048	-0.153207	4.816634
800.316204	8000.416424	12.439053	-0.153216	4.816639
799.878346	8000.457023	12.444058	-0.153135	4.816653
800.022308	8000.510288	12.449063	-0.153161	4.816668
800.131238	8000.303068	12.454067	-0.153182	4.816606
799.771252	8000.340694	12.459072	-0.153115	4.816619
799.484873	8000.470754	12.464077	-0.153061	4.816659
799.990188	8000.427002	12.469082	-0.153155	4.816643
799.876105	8000.493036	12.474087	-0.153134	4.816663
800.153910	8000.525143	12.479091	-0.153186	4.816671
800.501432	8000.414107	12.484096	-0.153250	4.816637
799.962873	8000.467917	12.489101	-0.153150	4.816655
800.120234	8000.271034	12.494106	-0.153179	4.816597
799.749387	8000.297875	12.499111	-0.153110	4.816606
799.995093	8000.309301	12.504115	-0.153156	4.816609
799.712373	8000.247405	12.509120	-0.153103	4.816592
799.391219	8000.058644	12.514125	-0.153043	4.816538
799.754458	8000.052886	12.519130	-0.153111	4.816534
799.776301	8000.325878	12.524135	-0.153115	4.816615
799.778607	8000.177392	12.529139	-0.153115	4.816571
800.227194	8000.353375	12.534144	-0.153199	4.816621
800.325846	8000.402719	12.539149	-0.153217	4.816635
800.252630	8000.349539	12.544154	-0.153203	4.816619
799.756491	8000.379642	12.549159	-0.153111	4.816631
800.228549	8000.406427	12.554163	-0.153199	4.816636
800.190500	8000.320934	12.559168	-0.153192	4.816611
799.838014	8000.131658	12.564173	-0.153126	4.816557
799.892808	7999.987211	12.569178	-0.153136	4.816514
799.776677	8000.308876	12.574183	-0.153115	4.816610
799.592638	8000.137198	12.579187	-0.153080	4.816560
799.876751	8000.118484	12.584192	-0.153133	4.816553
799.819421	8000.302136	12.589197	-0.153122	4.816607
799.716072	8000.025688	12.594202	-0.153103	4.816527
799.793053	8000.353681	12.599207	-0.153117	4.816623
799.612785	8000.272237	12.604211	-0.153084	4.816600
798.905099	8000.428319	12.609216	-0.152952	4.816649
800.017722	8000.345662	12.614221	-0.153159	4.816619
799.551796	8000.112105	12.619226	-0.153072	4.816553
799.784479	8000.176360	12.624231	-0.153116	4.816571
799.650910	8000.121139	12.629235	-0.153091	4.816555
799.214843	8000.143737	12.634240	-0.153009	4.816564
799.857821	8000.304848	12.639245	-0.153129	4.816608
799.685645	8000.261726	12.644250	-0.153097	4.816596
799.644585	8000.392601	12.649255	-0.153089	4.816635
799.906072	8000.266372	12.654259	-0.153138	4.816596
800.098807	8000.232378	12.659264	-0.153174	4.816586
800.054361	8000.417303	12.664269	-0.153166	4.816640
799.865227	8000.309191	12.669274	-0.153130	4.816609
799.537300	8000.154265	12.674279	-0.153069	4.816565
799.756378	8000.153586	12.679283	-0.153110	4.816564
800.369739	8000.468047	12.684288	-0.153224	4.816654
800.343310	8000.266045	12.689293	-0.153219	4.816594
800.520783	8000.490659	12.694298	-0.153252	4.816660
800.532198	8000.449467	12.699303	-0.153254	4.816647
800.583723	8000.520322	12.704307	-0.153264	4.816668
800.091824	8000.267238	12.709312	-0.153172	4.816596
800.067409	8000.358071	12.714317	-0.153168	4.816623
800.021764	8000.331863	12.719322	-0.153159	4.816615
800.003256	8000.336862	12.724327	-0.153156	4.816617
800.407338	8000.413462	12.729331	-0.153231	4.816637
800.696986	8000.370440	12.734336	-0.153285	4.816623
800.172600	8000.446760	12.739341	-0.153187	4.816648
799.984794	8000.063906	12.744346	-0.153152	4.816537
800.259475	8000.524553	12.749351	-0.153203	4.816671
800.221445	8000.193997	12.754355	-0.153196	4.816574
800.304920	8000.298258	12.759360	-0.153211	4.816604
800.422393	8000.344726	12.764365	-0.153233	4.816617
800.511090	8000.334498	12.769370	-0.153250	4.816614
800.293770	8000.315040	12.774375	-0.153209	4.816609
800.438712	8000.208128	12.779379	-0.153236	4.816577
800.829175	8000.523207	12.784384	-0.153309	4.816668
800.776327	8000.428983	12.789389	-0.153299	4.816640
800.462302	8000.344294	12.794394	-0.153241	4.816617
800.337775	8000.354992	12.799399	-0.153217	4.816621
800.599011	8000.315750	12.804403	-0.153266	4.816608
800.951386	8000.435006	12.809408	-0.153332	4.816641
800.908682	8000.526605	12.814413	-0.153324	4.816668
800.989065	8000.466379	12.819418	-0.153338	4.816650
800.682039	8000.432726	12.824423	-0.153281	4.816642
800.873027	8000.418862	12.829427	-0.153317	4.816637
800.683900	8000.458211	12.834432	-0.153282	4.816649
800.733734	8000.533283	12.839437	-0.153291	4.816671
801.118875	8000.467418	12.844442	-0.153362	4.816650
801.314378	8000.510917	12.849447	-0.153399	4.816662
801.194917	8000.451676	12.854451	-0.153377	4.816645
801.243239	8000.539455	12.859456	-0.153386	4.816670
800.963408	8000.445772	12.864461	-0.153333	4.816644
801.147103	8000.374501	12.869466	-0.153367	4.816622
801.219562	8000.392653	12.874471	-0.153381	4.816627
800.844158	8000.449122	12.879475	-0.153311	4.816646
801.454095	8000.543938	12.884480	-0.153425	4.816671
801.003279	8000.529156	12.889485	-0.153341	4.816669
800.654072	8000.346289	12.894490	-0.153275	4.816616
800.892811	8000.522043	12.899495	-0.153320	4.816667
801.264682	8000.475058	12.904499	-0.153389	4.816651
800.598670	8000.416455	12.909504	-0.153265	4.816637
800.547491	8000.429409	12.914509	-0.153255	4.816641
800.502100	8000.285446	12.919514	-0.153247	4.816599
800.767903	8000.438299	12.924519	-0.153296	4.816643
800.999079	8000.499354	12.929523	-0.153339	4.816660
800.783068	8000.479915	12.934528	-0.153299	4.816655
800.695822	8000.438175	12.939533	-0.153283	4.816643
800.932493	8000.411264	12.944538	-0.153327	4.816634
800.859923	8000.442965	12.949543	-0.153313	4.816644
801.025046	8000.543257	12.954547	-0.153344	4.816673
800.629284	8000.353266	12.959552	-0.153270	4.816619
800.768235	8000.430850	12.964557	-0.153296	4.816641
801.409999	8000.534671	12.969562	-0.153416	4.816668
801.152018	8000.530461	12.974567	-0.153368	4.816668
801.124631	8000.482270	12.979571	-0.153362	4.816654
800.901455	8000.354502	12.984576	-0.153321	4.816618
800.803758	8000.364576	12.989581	-0.153303	4.816621
801.131953	8000.461160	12.994586	-0.153364	4.816648
801.057095	8000.442962	12.999591	-0.153350	4.816643
800.942722	8000.337126	13.004595	-0.153328	4.816612
801.024838	8000.560189	13.009600	-0.153344	4.816678
800.553501	8000.360479	13.014605	-0.153256	4.816621
800.908428	8000.454315	13.019610	-0.153322	4.816647
800.987989	8000.434391	13.024615	-0.153337	4.816641
801.190013	8000.455717	13.029619	-0.153374	4.816646
801.287125	8000.511404	13.034624	-0.153392	4.816662
801.192430	8000.441958	13.039629	-0.153375	4.816642
801.401834	8000.555704	13.044634	-0.153414	4.816675
800.860983	8000.246647	13.049639	-0.153313	4.816586
800.791831	8000.185046	13.054643	-0.153300	4.816568
801.131105	8000.499293	13.059648	-0.153363	4.816659
800.630220	8000.373364	13.064653	-0.153270	4.816625
800.863504	8000.341093	13.069658	-0.153313	4.816614
801.109106	8000.397077	13.074663	-0.153359	4.816629
801.401298	8000.465493	13.079667	-0.153413	4.816648
801.089381	8000.466768	13.084672	-0.153355	4.816650
801.328539	8000.522649	13.089677	-0.153400	4.816665
801.599755	8000.461292	13.094682	-0.153450	4.816646
800.766310	8000.230217	13.099687	-0.153295	4.816582
800.821323	8000.157909	13.104691	-0.153305	4.816560
801.106486	8000.468091	13.109696	-0.153358	4.816650
801.069935	8000.448395	13.114701	-0.153351	4.816645
801.108898	8000.276100	13.119706	-0.153358	4.816594
801.268654	8000.487699	13.124711	-0.153388	4.816655
801.152939	8000.421093	13.129715	-0.153366	4.816636
800.574210	8000.110365	13.134720	-0.153258	4.816547
800.608568	8000.145930	13.139725	-0.153265	4.816558
800.484621	7999.856414	13.144730	-0.153242	4.816473
800.943274	8000.285049	13.149735	-0.153327	4.816597
801.263258	8000.392108	13.154739	-0.153387	4.816627
801.665924	8000.424133	13.159744	-0.153462	4.816635
801.140757	8000.244761	13.164749	-0.153364	4.816584
801.340723	8000.360473	13.169754	-0.153401	4.816617
801.091131	8000.324573	13.174759	-0.153355	4.816608
801.220264	8000.288483	13.179763	-0.153379	4.816597
801.264031	8000.240391	13.184768	-0.153387	4.816582
800.978276	8000.417143	13.189773	-0.153333	4.816636
800.952960	8000.151504	13.194778	-0.153329	4.816558
801.010750	8000.333854	13.199783	-0.153339	4.816611
800.935951	8000.163950	13.204787	-0.153325	4.816562
801.406018	8000.310586	13.209792	-0.153413	4.816602
800.951672	8000.271349	13.214797	-0.153328	4.816593
801.119321	8000.368498	13.219802	-0.153359	4.816621
801.234136	8000.486005	13.224807	-0.153381	4.816655
800.679718	8000.026088	13.229811	-0.153277	4.816522
801.144098	8000.240523	13.234816	-0.153364	4.816583
800.748527	8000.235133	13.239821	-0.153290	4.816583
800.905531	7999.855774	13.244826	-0.153319	4.816471
801.227676	8000.408436	13.249831	-0.153379	4.816632
801.084986	8000.249094	13.254835	-0.153353	4.816586
801.087404	7999.919196	13.259840	-0.153353	4.816489
801.237805	8000.303561	13.264845	-0.153381	4.816601
800.917151	8000.061754	13.269850	-0.153321	4.816532
800.780090	8000.150752	13.274855	-0.153296	4.816558
801.067549	8000.268949	13.279859	-0.153349	4.816592
800.479458	8000.133116	13.284864	-0.153240	4.816555
800.645584	8000.366031	13.289869	-0.153271	4.816622
801.049988	8000.171050	13.294874	-0.153346	4.816563
800.768165	7999.927758	13.299879	-0.153293	4.816493
800.728071	8000.336599	13.304883	-0.153286	4.816613
800.801848	8000.083187	13.309888	-0.153299	4.816538
800.439972	7999.867237	13.314893	-0.153232	4.816477
800.597140	7999.904802	13.319898	-0.153261	4.816487
800.780464	8000.299247	13.324903	-0.153295	4.816602
800.877569	8000.266878	13.329907	-0.153313	4.816592
801.198967	8000.239226	13.334912	-0.153373	4.816582
801.070817	8000.462043	13.339917	-0.153350	4.816649
800.790351	8000.175271	13.344922	-0.153297	4.816566
800.755132	8000.283964	13.349927	-0.153291	4.816598
800.717508	8000.031920	13.354931	-0.153283	4.816524
801.137380	8000.118324	13.359936	-0.153362	4.816547
801.257302	8000.468249	13.364941	-0.153384	4.816650
800.868165	8000.196678	13.369946	-0.153311	4.816571
801.015850	8000.353972	13.374951	-0.153339	4.816617
801.057437	8000.330245	13.379955	-0.153347	4.816610
801.121224	8000.191244	13.384960	-0.153358	4.816569
801.095080	8000.551520	13.389965	-0.153354	4.816675
801.378859	8000.343962	13.394970	-0.153406	4.816612
801.116690	8000.203890	13.399975	-0.153357	4.816572
800.975045	8000.030777	13.404979	-0.153331	4.816522
801.523276	8000.479982	13.409984	-0.153433	4.816652
802.045883	8000.510782	13.414989	-0.153531	4.816658
802.192763	8000.508931	13.419994	-0.153558	4.816657
801.978478	8000.475725	13.424999	-0.153518	4.816648
801.713325	8000.409864	13.430003	-0.153468	4.816630
801.900452	8000.465958	13.435008	-0.153503	4.816646
801.878499	8000.407246	13.440013	-0.153499	4.816629
801.688286	8000.547364	13.445018	-0.153464	4.816671
802.010890	8000.519735	13.450023	-0.153524	4.816661
801.667053	8000.464259	13.455027	-0.153460	4.816646
801.706150	8000.552950	13.460032	-0.153467	4.816672
801.790368	8000.445045	13.465037	-0.153482	4.816640
802.181940	8000.547974	13.470042	-0.153555	4.816669
801.750972	8000.446517	13.475047	-0.153475	4.816641
801.965432	8000.462743	13.480051	-0.153515	4.816645
802.079555	8000.448687	13.485056	-0.153536	4.816640
801.495612	8000.355348	13.490061	-0.153427	4.816615
802.080496	8000.527204	13.495066	-0.153536	4.816663
801.814222	8000.527101	13.500071	-0.153487	4.816664
801.395637	8000.420544	13.505075	-0.153409	4.816635
801.657176	8000.414197	13.510080	-0.153457	4.816632
801.750643	8000.373281	13.515085	-0.153475	4.816619
802.179885	8000.417410	13.520090	-0.153555	4.816630
802.437586	8000.444951	13.525095	-0.153603	4.816637
802.722164	8000.443225	13.530099	-0.153655	4.816635
802.692621	8000.517006	13.535104	-0.153650	4.816657
802.317653	8000.508762	13.540109	-0.153580	4.816656
802.216689	8000.538940	13.545114	-0.153561	4.816666
802.307668	8000.505409	13.550119	-0.153578	4.816655
802.003691	8000.438913	13.555123	-0.153521	4.816637
802.016472	8000.546272	13.560128	-0.153524	4.816669
801.934601	8000.525836	13.565133	-0.153509	4.816663
801.694456	8000.260930	13.570138	-0.153464	4.816586
802.223669	8000.455219	13.575143	-0.153562	4.816641
802.486329	8000.488145	13.580147	-0.153611	4.816650
802.256679	8000.503492	13.585152	-0.153568	4.816655
801.737953	8000.504575	13.590157	-0.153472	4.816658
802.044254	8000.449095	13.595162	-0.153529	4.816640
802.462378	8000.496228	13.600167	-0.153607	4.816652
802.547329	8000.537927	13.605171	-0.153622	4.816664
802.681881	8000.525265	13.610176	-0.153647	4.816660
802.485347	8000.510385	13.615181	-0.153611	4.816656
802.581038	8000.507699	13.620186	-0.153629	4.816655
802.283841	8000.525126	13.625191	-0.153573	4.816661
801.896245	8000.501824	13.630195	-0.153501	4.816656
801.796937	8000.463069	13.635200	-0.153482	4.816645
801.640933	8000.440363	13.640205	-0.153453	4.816640
801.779637	8000.513704	13.645210	-0.153479	4.816660
802.123458	8000.517187	13.650215	-0.153543	4.816660
801.991126	8000.452430	13.655219	-0.153518	4.816641
801.580855	8000.275989	13.660224	-0.153442	4.816591
801.984014	8000.541425	13.665229	-0.153517	4.816668
801.911377	8000.427778	13.670234	-0.153503	4.816635
802.029239	8000.467891	13.675239	-0.153525	4.816646
802.149623	8000.461363	13.680243	-0.153548	4.816643
802.038600	8000.386345	13.685248	-0.153527	4.816622
801.693178	8000.364794	13.690253	-0.153463	4.816617
801.845621	8000.330145	13.695258	-0.153491	4.816606
801.999765	8000.453600	13.700263	-0.153520	4.816642
802.284532	8000.517654	13.705267	-0.153573	4.816659
802.224375	8000.386175	13.710272	-0.153561	4.816621
801.998972	8000.550121	13.715277	-0.153519	4.816670
801.763545	8000.224820	13.720282	-0.153475	4.816576
801.422860	8000.182131	13.725287	-0.153412	4.816565
801.634012	8000.335157	13.730291	-0.153451	4.816609
801.962635	8000.339451	13.735296	-0.153512	4.816608
802.102460	8000.452065	13.740301	-0.153538	4.816641
801.953782	8000.401894	13.745306	-0.153511	4.816627
802.038487	8000.469050	13.750311	-0.153526	4.816646
802.298171	8000.469039	13.755315	-0.153575	4.816645
801.963049	8000.393548	13.760320	-0.153512	4.816624
801.517743	8000.421292	13.765325	-0.153429	4.816635
802.027287	8000.247121	13.770330	-0.153524	4.816581
801.680211	8000.248884	13.775335	-0.153459	4.816583
801.939324	8000.441949	13.780339	-0.153508	4.816639
801.881236	8000.437815	13.785344	-0.153497	4.816638
802.017097	8000.545060	13.790349	-0.153522	4.816669
802.271162	8000.518434	13.795354	-0.153569	4.816660
802.344041	8000.431562	13.800359	-0.153583	4.816634
802.550016	8000.521916	13.805363	-0.153621	4.816659
802.344843	8000.475066	13.810368	-0.153583	4.816646
802.331322	8000.402699	13.815373	-0.153580	4.816625
802.260130	8000.474738	13.820378	-0.153567	4.816647
801.825746	8000.435821	13.825383	-0.153486	4.816637
801.992150	8000.424740	13.830387	-0.153517	4.816633
802.118843	8000.426803	13.835392	-0.153541	4.816633
802.190057	8000.471459	13.840397	-0.153554	4.816646
802.517693	8000.533031	13.845402	-0.153615	4.816663
802.766509	8000.539209	13.850407	-0.153661	4.816663
802.544600	8000.528158	13.855411	-0.153620	4.816661
802.507753	8000.473445	13.860416	-0.153613	4.816645
802.350100	8000.532404	13.865421	-0.153584	4.816663
802.976071	8000.507604	13.870426	-0.153700	4.816653
802.832245	8000.538143	13.875431	-0.153673	4.816663
802.512989	8000.510650	13.880435	-0.153614	4.816656
802.619742	8000.461463	13.885440	-0.153634	4.816641
802.455821	8000.529868	13.890445	-0.153603	4.816662
802.294307	8000.374455	13.895450	-0.153573	4.816617
802.413537	8000.458088	13.900455	-0.153595	4.816641
802.496192	8000.557039	13.905459	-0.153610	4.816670
802.278894	8000.246882	13.910464	-0.153570	4.816580
801.851389	8000.488162	13.915469	-0.153490	4.816653
802.102940	8000.461494	13.920474	-0.153537	4.816644
802.438216	8000.451046	13.925479	-0.153599	4.816639
802.357758	8000.535666	13.930483	-0.153584	4.816664
802.348871	8000.246945	13.935488	-0.153583	4.816579
802.241111	8000.527390	13.940493	-0.153563	4.816662
802.437807	8000.454209	13.945498	-0.153599	4.816640
801.936756	8000.390864	13.950503	-0.153506	4.816624
801.941350	8000.397301	13.955507	-0.153507	4.816626
802.320173	8000.415146	13.960512	-0.153577	4.816629
801.952526	8000.470679	13.965517	-0.153509	4.816647
801.894368	8000.351965	13.970522	-0.153498	4.816612
801.888434	8000.327464	13.975527	-0.153497	4.816605
801.664861	8000.477647	13.980531	-0.153455	4.816650
802.076227	8000.464196	13.985536	-0.153532	4.816645
802.187836	8000.494658	13.990541	-0.153552	4.816653
802.568194	8000.537993	13.995546	-0.153623	4.816664
802.391500	8000.468268	14.000551	-0.153590	4.816644
802.289033	8000.509030	14.005555	-0.153571	4.816657
801.962105	8000.353042	14.010560	-0.153510	4.816612
801.790022	8000.432983	14.015565	-0.153478	4.816637
801.822236	8000.347571	14.020570	-0.153484	4.816611
801.736741	8000.299493	14.025575	-0.153468	4.816598
801.567261	8000.324310	14.030579	-0.153436	4.816606
801.244344	7999.860740	14.035584	-0.153376	4.816471
801.456093	8000.053023	14.040589	-0.153415	4.816527
801.358136	7999.853039	14.045594	-0.153397	4.816468
801.556684	8000.029194	14.050599	-0.153434	4.816519
801.750557	8000.149049	14.055603	-0.153470	4.816553
801.908004	7999.942616	14.060608	-0.153499	4.816492
802.032403	8000.480400	14.065613	-0.153523	4.816650
802.384479	8000.475530	14.070618	-0.153588	4.816646
802.354768	8000.402899	14.075623	-0.153583	4.816625
802.257918	8000.485129	14.080627	-0.153565	4.816650
801.654899	8000.078511	14.085632	-0.153452	4.816533
801.666993	8000.382122	14.090637	-0.153454	4.816622
801.859518	8000.482863	14.095642	-0.153490	4.816651
801.875744	8000.354753	14.100647	-0.153493	4.816613
801.843816	8000.391361	14.105651	-0.153487	4.816624
802.156832	8000.378427	14.110656	-0.153546	4.816619
801.982614	8000.514563	14.115661	-0.153513	4.816660
801.619671	8000.274178	14.120666	-0.153445	4.816591
801.698467	8000.338053	14.125671	-0.153460	4.816609
801.851066	8000.498615	14.130675	-0.153489	4.816656
801.832903	8000.375248	14.135680	-0.153485	4.816620
802.073125	8000.366431	14.140685	-0.153530	4.816616
802.550726	8000.546090	14.145690	-0.153619	4.816666
802.634480	8000.450908	14.150695	-0.153634	4.816638
802.597135	8000.508647	14.155699	-0.153627	4.816655
802.664726	8000.555367	14.160704	-0.153640	4.816669
802.460889	8000.530818	14.165709	-0.153602	4.816662
802.617533	8000.523822	14.170714	-0.153631	4.816660
802.220143	8000.364561	14.175719	-0.153557	4.816615
802.065030	8000.356723	14.180723	-0.153528	4.816613
802.229347	8000.417751	14.185728	-0.153558	4.816630
801.845496	8000.357379	14.190733	-0.153487	4.816614
801.545412	8000.181677	14.195738	-0.153431	4.816564
801.147205	7999.836764	14.200743	-0.153356	4.816464
801.430107	7999.864708	14.205747	-0.153409	4.816471
801.587811	7999.899101	14.210752	-0.153438	4.816481
801.407764	7999.964060	14.215757	-0.153405	4.816501
801.194584	7999.989226	14.220762	-0.153365	4.816509
801.820187	7999.934704	14.225767	-0.153482	4.816490
801.783512	8000.279955	14.230771	-0.153475	4.816592
801.724996	7999.963911	14.235776	-0.153464	4.816499
802.080904	8000.346331	14.240781	-0.153530	4.816610
802.056156	8000.457320	14.245786	-0.153526	4.816643
801.856315	8000.234448	14.250791	-0.153488	4.816578
801.818884	8000.196702	14.255795	-0.153481	4.816567
801.903045	7999.536079	14.260800	-0.153497	4.816372

801.511672	7996.295481	14.265805	-0.153421	4.815420
801.614253	7990.656543	14.270810	-0.153437	4.813760
802.126429	7984.026576	14.275815	-0.153528	4.811805
801.707170	7976.702228	14.280819	-0.153445	4.809649
801.691686	7969.151466	14.285824	-0.153437	4.807423
801.479176	7961.260392	14.290829	-0.153392	4.805097
801.297497	7953.438224	14.295834	-0.153353	4.802790
801.875822	7945.438834	14.300839	-0.153456	4.800426
801.995478	7937.436396	14.305843	-0.153473	4.798062
802.257165	7929.468457	14.310848	-0.153516	4.795706
801.705269	7921.506359	14.315853	-0.153408	4.793355
801.478303	7913.554056	14.320858	-0.153361	4.791004
802.020849	7905.462533	14.325863	-0.153457	4.788607
801.837004	7897.420709	14.330867	-0.153417	4.786227
801.803119	7889.438743	14.335872	-0.153406	4.783862
802.180564	7881.496804	14.340877	-0.153471	4.781507
802.003745	7873.438682	14.345882	-0.153432	4.779118
801.944615	7865.528234	14.350887	-0.153416	4.776772
801.053049	7857.456441	14.355891	-0.153245	4.774380
801.614458	7849.514609	14.360896	-0.153344	4.772019
801.495962	7841.439878	14.365901	-0.153317	4.769620
801.687278	7833.412957	14.370906	-0.153347	4.767234
801.892271	7825.415344	14.375911	-0.153380	4.764854
801.694128	7817.431561	14.380915	-0.153338	4.762479
801.826983	7809.430543	14.385920	-0.153357	4.760097
801.285060	7801.523207	14.390925	-0.153251	4.757744
801.310690	7793.408542	14.395930	-0.153251	4.755325
801.356230	7785.443735	14.400935	-0.153254	4.752950
801.101119	7777.433592	14.405939	-0.153201	4.750562
801.064085	7769.407953	14.410944	-0.153189	4.748167
801.026098	7761.385331	14.415949	-0.153177	4.745771
800.883191	7753.413761	14.420954	-0.153145	4.743390
801.409054	7745.388271	14.425959	-0.153238	4.740989
801.178977	7737.411349	14.430963	-0.153190	4.738604
800.816380	7729.482107	14.435968	-0.153117	4.736233
800.747070	7721.381490	14.440973	-0.153099	4.733808
800.879317	7713.374471	14.445978	-0.153118	4.731410
800.943330	7705.386472	14.450983	-0.153125	4.729016
800.815449	7697.313343	14.455987	-0.153095	4.726595
800.855643	7689.379056	14.460992	-0.153098	4.724215
800.642528	7681.466356	14.465997	-0.153053	4.721841
801.076307	7673.312625	14.471002	-0.153128	4.719391
800.347369	7665.498402	14.476007	-0.152987	4.717045
800.653133	7657.347697	14.481011	-0.153039	4.714595
800.996111	7649.402747	14.486016	-0.153098	4.712205
800.940382	7641.314503	14.491021	-0.153082	4.709771
800.448881	7633.402471	14.496026	-0.152985	4.707390
800.263615	7625.392178	14.501031	-0.152946	4.704978
800.355881	7617.355904	14.506035	-0.152957	4.702556
800.450783	7609.359992	14.511040	-0.152970	4.700145
800.657681	7601.341993	14.516045	-0.153003	4.697725
800.084713	7593.337543	14.521050	-0.152891	4.695310
800.021839	7585.359207	14.526055	-0.152874	4.692901
799.956002	7577.299244	14.531059	-0.152857	4.690466
800.065488	7569.358092	14.536064	-0.152872	4.688065
799.813600	7561.310591	14.541069	-0.152820	4.685632
800.299386	7553.298190	14.546074	-0.152905	4.683206
800.128867	7545.416224	14.551079	-0.152868	4.680820
799.832589	7537.356377	14.556083	-0.152807	4.678379
800.019526	7529.397939	14.561088	-0.152837	4.675966
800.011522	7521.341771	14.566093	-0.152830	4.673524
799.752160	7513.288710	14.571098	-0.152777	4.671081
799.937388	7505.294298	14.576103	-0.152806	4.668654
799.785858	7497.226569	14.581107	-0.152772	4.666203
800.093134	7489.227569	14.586112	-0.152824	4.663772
799.616248	7481.376556	14.591117	-0.152730	4.661386
799.643719	7473.304751	14.596122	-0.152730	4.658930
799.651530	7465.340711	14.601127	-0.152726	4.656506
799.359775	7457.276379	14.606131	-0.152667	4.654051
799.148947	7449.428713	14.611136	-0.152622	4.651660
798.747359	7441.336880	14.616141	-0.152542	4.649194
799.053861	7433.349510	14.621146	-0.152594	4.646757
798.815670	7425.355762	14.626151	-0.152545	4.644318
798.905370	7417.363937	14.631155	-0.152556	4.641878
799.008401	7409.350772	14.636160	-0.152570	4.639430
799.037013	7401.327380	14.641165	-0.152570	4.636978
799.043262	7393.240835	14.646170	-0.152566	4.634505
799.180728	7385.299559	14.651175	-0.152586	4.632075
798.951747	7377.264113	14.656179	-0.152538	4.629615
799.407801	7369.318254	14.661184	-0.152618	4.627181
799.136260	7361.316797	14.666189	-0.152562	4.624729
798.873183	7353.352275	14.671194	-0.152508	4.622287
798.772313	7345.346349	14.676199	-0.152484	4.619831
799.018563	7337.298007	14.681203	-0.152524	4.617361
799.171500	7329.263035	14.686208	-0.152548	4.614893
798.823088	7321.322830	14.691213	-0.152478	4.612453
799.263715	7313.248563	14.696218	-0.152554	4.609971
798.900390	7305.362637	14.701223	-0.152482	4.607545
798.592637	7297.273073	14.706227	-0.152419	4.605055
798.346390	7289.365326	14.711232	-0.152368	4.602620
798.310108	7281.289400	14.716237	-0.152356	4.600132
798.592455	7273.272091	14.721242	-0.152403	4.597660
798.445546	7265.306228	14.726247	-0.152371	4.595203
798.230755	7257.318517	14.731251	-0.152325	4.592738
798.666939	7249.271219	14.736256	-0.152401	4.590254
798.467653	7241.254762	14.741261	-0.152359	4.587777
798.116883	7233.224905	14.746266	-0.152288	4.585295
798.551450	7225.280275	14.751271	-0.152364	4.582838
798.232207	7217.209697	14.756275	-0.152299	4.580340
798.499483	7209.277003	14.761280	-0.152344	4.577885
798.267400	7201.274478	14.766285	-0.152295	4.575406
798.222343	7193.265693	14.771290	-0.152282	4.572923
798.075626	7185.274728	14.776295	-0.152249	4.570445
797.868725	7177.263241	14.781299	-0.152205	4.567959
798.117866	7169.212183	14.786304	-0.152246	4.565460
797.826996	7161.269162	14.791309	-0.152187	4.562992
797.605395	7153.265989	14.796314	-0.152140	4.560505
797.639746	7145.324334	14.801319	-0.152142	4.558035
797.717878	7137.209212	14.806323	-0.152151	4.555510
797.925066	7129.258350	14.811328	-0.152184	4.553035
797.578923	7121.283501	14.816333	-0.152115	4.550551
797.690660	7113.178524	14.821338	-0.152130	4.548025
797.598705	7105.215263	14.826343	-0.152108	4.545542
797.458387	7097.207654	14.831347	-0.152076	4.543043
797.250309	7089.247906	14.836352	-0.152032	4.540558
797.174231	7081.269818	14.841357	-0.152013	4.538066
796.822797	7073.249941	14.846362	-0.151942	4.535559
797.316098	7065.186253	14.851367	-0.152029	4.533039
797.167032	7057.193002	14.856371	-0.151996	4.530538
796.688999	7049.265318	14.861376	-0.151902	4.528055
797.118186	7041.226155	14.866381	-0.151976	4.525538
796.551813	7033.268245	14.871386	-0.151866	4.523043
796.453513	7025.246768	14.876391	-0.151842	4.520528
795.924364	7017.282840	14.881395	-0.151738	4.518028
796.197513	7009.228754	14.886400	-0.151784	4.515501
795.599668	7001.235766	14.891405	-0.151667	4.512989
795.998198	6993.108169	14.896410	-0.151736	4.510435
796.286801	6985.114991	14.901415	-0.151785	4.507923
796.306556	6977.076896	14.906419	-0.151783	4.505394
796.144843	6969.149023	14.911424	-0.151748	4.502898
795.688789	6961.244125	14.916429	-0.151658	4.500407
795.260701	6953.208843	14.921434	-0.151573	4.497873
795.077495	6945.178932	14.926439	-0.151533	4.495341
794.948872	6937.153103	14.931443	-0.151504	4.492808
795.311515	6929.114192	14.936448	-0.151566	4.490272
795.558386	6921.082822	14.941453	-0.151607	4.487736
795.657992	6913.075180	14.946458	-0.151620	4.485205
795.615821	6905.185032	14.951463	-0.151607	4.482710
795.429699	6897.149893	14.956467	-0.151567	4.480167
795.483435	6889.178927	14.961472	-0.151572	4.477644
795.369267	6881.169941	14.966477	-0.151545	4.475107
795.120681	6873.167051	14.971482	-0.151494	4.472570
795.325831	6865.109524	14.976487	-0.151527	4.470015
794.687613	6857.169557	14.981491	-0.151403	4.467493
794.731169	6849.082793	14.986496	-0.151406	4.464926
795.465780	6841.102464	14.991501	-0.151537	4.462394
794.644052	6833.152141	14.996506	-0.151379	4.459864
795.288742	6825.113996	15.001511	-0.151494	4.457310
795.402468	6817.054492	15.006515	-0.151510	4.454746
795.419133	6809.150812	15.011520	-0.151507	4.452230
795.327308	6801.075669	15.016525	-0.151485	4.449657
794.780927	6793.124784	15.021530	-0.151378	4.447120
795.011974	6785.063607	15.026535	-0.151416	4.444550
794.743828	6777.139915	15.031539	-0.151361	4.442020
794.679222	6769.102722	15.036544	-0.151343	4.439454
794.694976	6761.159947	15.041549	-0.151341	4.436916
794.381108	6753.080886	15.046554	-0.151277	4.434332
794.449860	6745.130980	15.051559	-0.151285	4.431790
794.557899	6737.064125	15.056563	-0.151300	4.429208
794.618824	6729.060131	15.061568	-0.151306	4.426646
794.125286	6721.086532	15.066573	-0.151209	4.424088
794.443039	6713.088007	15.071578	-0.151263	4.421525
794.533544	6705.045903	15.076583	-0.151274	4.418946
794.656318	6697.050752	15.081587	-0.151292	4.416380
794.595376	6689.044616	15.086592	-0.151275	4.413809
794.241832	6681.118713	15.091597	-0.151204	4.411260
794.191590	6673.004368	15.096602	-0.151189	4.408651
794.242544	6665.079470	15.101607	-0.151194	4.406101
794.018285	6657.042476	15.106611	-0.151147	4.403513
794.091336	6649.091601	15.111616	-0.151155	4.400952
794.339375	6641.056205	15.116621	-0.151196	4.398364
794.014046	6633.077783	15.121626	-0.151130	4.395789
794.251486	6625.061607	15.126631	-0.151169	4.393204
793.376806	6617.105177	15.131635	-0.151001	4.390630
793.929771	6609.001130	15.136640	-0.151099	4.388015
794.364636	6600.941457	15.141645	-0.151174	4.385412
794.077682	6592.987194	15.146650	-0.151116	4.382838
794.120279	6585.054882	15.151655	-0.151118	4.380271
793.791889	6577.053066	15.156659	-0.151052	4.377678
793.685700	6569.084755	15.161664	-0.151027	4.375095
793.738261	6561.120147	15.166669	-0.151032	4.372513
793.648427	6553.000336	15.171674	-0.151010	4.369878
793.451296	6545.086554	15.176679	-0.150968	4.367308
793.112743	6537.084159	15.181683	-0.150899	4.364707
793.127838	6529.120102	15.186688	-0.150897	4.362119
793.477009	6521.022691	15.191693	-0.150957	4.359488
793.471079	6513.062769	15.196698	-0.150950	4.356898
793.233833	6505.038431	15.201703	-0.150901	4.354284
793.196703	6497.010159	15.206707	-0.150889	4.351668
793.059621	6489.006022	15.211712	-0.150858	4.349058
793.343641	6480.975066	15.216717	-0.150905	4.346441
793.431892	6472.948152	15.221722	-0.150917	4.343822
793.212745	6465.096929	15.226727	-0.150871	4.341257
792.932754	6457.039686	15.231731	-0.150813	4.338622
792.891888	6449.075871	15.236736	-0.150800	4.336018
792.880633	6441.050395	15.241741	-0.150793	4.333392
792.911821	6432.994543	15.246746	-0.150794	4.330755
792.792972	6425.095551	15.251751	-0.150766	4.328167
793.050533	6417.033925	15.256755	-0.150809	4.325527
792.919366	6409.091497	15.261760	-0.150779	4.322921
792.624093	6401.133859	15.266765	-0.150719	4.320308
792.781096	6393.074821	15.271770	-0.150743	4.317663
792.488568	6385.141223	15.276775	-0.150683	4.315054
792.534416	6377.118290	15.281779	-0.150687	4.312417
792.302526	6369.090634	15.286784	-0.150638	4.309775
792.439949	6361.101946	15.291789	-0.150658	4.307146
792.349370	6353.000327	15.296794	-0.150636	4.304477
792.394507	6345.090873	15.301799	-0.150639	4.301871
791.955721	6337.057845	15.306803	-0.150553	4.299218
791.850106	6329.120197	15.311808	-0.150528	4.296598
792.215489	6320.986792	15.316813	-0.150590	4.293916
792.124019	6313.019869	15.321818	-0.150568	4.291283
791.751304	6305.077184	15.326823	-0.150493	4.288655
791.830250	6297.059270	15.331827	-0.150503	4.286003
791.686885	6289.038737	15.336832	-0.150471	4.283347
791.774897	6281.050309	15.341837	-0.150482	4.280702
791.610258	6273.029980	15.346842	-0.150446	4.278043
791.370840	6265.117364	15.351847	-0.150396	4.275417
791.424308	6257.058136	15.356851	-0.150401	4.272743
791.789731	6249.003235	15.361856	-0.150464	4.270072
791.599902	6241.024346	15.366861	-0.150423	4.267420
791.634852	6232.971260	15.371866	-0.150424	4.264743
791.815427	6225.078803	15.376871	-0.150453	4.262119
791.280435	6217.077411	15.381875	-0.150348	4.259451
791.153222	6209.083230	15.386880	-0.150319	4.256787
790.769133	6201.126471	15.391885	-0.150242	4.254132
790.566733	6193.101485	15.396890	-0.150199	4.251454
790.913417	6185.026096	15.401895	-0.150259	4.248763
791.332765	6176.938693	15.406899	-0.150331	4.246066
790.758966	6169.066535	15.411904	-0.150219	4.243430
791.109135	6161.028472	15.416909	-0.150279	4.240746
791.245156	6152.991247	15.421914	-0.150299	4.238059
791.339251	6145.046061	15.426919	-0.150312	4.235400
791.122371	6137.041269	15.431923	-0.150266	4.232717
791.111096	6129.051459	15.436928	-0.150259	4.230039
790.943429	6121.073192	15.441933	-0.150222	4.227362
790.981437	6113.014905	15.446938	-0.150224	4.224658
790.695555	6105.128510	15.451943	-0.150166	4.222006
791.053002	6097.017014	15.456947	-0.150227	4.219284
790.774617	6089.099715	15.461952	-0.150170	4.216619
791.044935	6081.001079	15.466957	-0.150215	4.213897
790.484818	6073.082274	15.471962	-0.150105	4.211225
790.745154	6065.081356	15.476967	-0.150148	4.208533
790.145322	6057.087160	15.481971	-0.150032	4.205832
790.224338	6049.079001	15.486976	-0.150041	4.203131
790.286211	6041.073730	15.491981	-0.150047	4.200430
790.227799	6033.033042	15.496986	-0.150031	4.197713
789.954686	6025.061674	15.501991	-0.149975	4.195016
790.225855	6016.989537	15.506995	-0.150020	4.192289
790.501420	6008.903962	15.512000	-0.150066	4.189556
789.940317	6001.057114	15.517005	-0.149957	4.186892
789.858505	5992.980667	15.522010	-0.149936	4.184155
790.035283	5985.050176	15.527015	-0.149964	4.181467
790.101041	5976.997763	15.532019	-0.149971	4.178736
789.807048	5969.018607	15.537024	-0.149911	4.176024
789.709530	5961.013402	15.542029	-0.149887	4.173303
789.719971	5953.001580	15.547034	-0.149884	4.170579
789.989420	5945.001845	15.552039	-0.149929	4.167861
789.453505	5937.024492	15.557043	-0.149824	4.165139
789.867574	5929.008223	15.562048	-0.149896	4.162413
789.836835	5921.010491	15.567053	-0.149885	4.159687
789.465603	5913.048085	15.572058	-0.149810	4.156967
789.657475	5905.012053	15.577063	-0.149841	4.154226
789.317577	5897.079331	15.582067	-0.149772	4.151513
789.597684	5888.998659	15.587072	-0.149819	4.148754
789.368391	5881.022470	15.592077	-0.149771	4.146024
789.578886	5872.934785	15.597082	-0.149805	4.143259
789.572716	5865.013272	15.602087	-0.149799	4.140546
789.190950	5857.066728	15.607091	-0.149723	4.137818
788.755801	5849.087470	15.612096	-0.149636	4.135077
788.991968	5841.045662	15.617101	-0.149675	4.132321
788.918868	5832.994966	15.622106	-0.149656	4.129555
788.815329	5825.077987	15.627111	-0.149632	4.126834
789.014799	5816.981723	15.632115	-0.149663	4.124053
789.111992	5809.049760	15.637120	-0.149676	4.121325
789.191202	5801.031218	15.642125	-0.149686	4.118566
788.796111	5793.089245	15.647130	-0.149607	4.115825
788.828407	5785.075982	15.652135	-0.149608	4.113062
788.394290	5777.071278	15.657139	-0.149522	4.110295
788.013798	5769.090001	15.662144	-0.149446	4.107535
787.740613	5761.109248	15.667149	-0.149389	4.104775
787.576471	5753.111735	15.672154	-0.149354	4.102008
788.180071	5744.987170	15.677159	-0.149461	4.099206
788.292371	5737.050195	15.682163	-0.149476	4.096460
788.119879	5729.013383	15.687168	-0.149439	4.093674
787.682200	5721.083466	15.692173	-0.149352	4.090919
787.750764	5713.037446	15.697178	-0.149360	4.088130
787.594542	5705.097519	15.702183	-0.149325	4.085372
787.623631	5697.087357	15.707187	-0.149326	4.082590
788.116553	5688.982381	15.712192	-0.149412	4.079780
787.876061	5681.106997	15.717197	-0.149362	4.077037
787.777156	5673.018772	15.722202	-0.149338	4.074221
788.043552	5665.037858	15.727207	-0.149383	4.071445
788.406343	5656.971488	15.732211	-0.149445	4.068639
787.923579	5649.048098	15.737216	-0.149350	4.065869
787.850787	5641.089293	15.742221	-0.149331	4.063090
787.555578	5633.068315	15.747226	-0.149271	4.060285
787.822012	5625.106471	15.752231	-0.149315	4.057506
787.642754	5617.026691	15.757235	-0.149277	4.054678
787.384429	5609.081693	15.762240	-0.149223	4.051894
787.555545	5601.032379	15.767245	-0.149250	4.049078
787.510752	5593.037819	15.772250	-0.149236	4.046275
787.448863	5585.047771	15.777255	-0.149219	4.043472
787.431447	5577.090743	15.782259	-0.149211	4.040680
786.759202	5569.171782	15.787264	-0.149081	4.037889
787.098371	5561.072882	15.792269	-0.149138	4.035048
787.001075	5553.018866	15.797274	-0.149115	4.032214
786.994561	5544.986122	15.802279	-0.149109	4.029387
786.947142	5536.978537	15.807283	-0.149095	4.026566
786.989053	5529.002779	15.812288	-0.149097	4.023756
787.334318	5521.003277	15.817293	-0.149156	4.020940
787.152589	5513.000744	15.822298	-0.149117	4.018113
786.993419	5505.049760	15.827303	-0.149082	4.015303
786.769195	5497.092311	15.832307	-0.149035	4.012487
786.765413	5489.042410	15.837312	-0.149029	4.009640
786.786815	5481.057948	15.842317	-0.149028	4.006815
786.733545	5473.015523	15.847322	-0.149013	4.003966
786.856810	5465.149588	15.852327	-0.149031	4.001180
786.999300	5457.015417	15.857331	-0.149052	3.998297
786.702832	5449.069860	15.862336	-0.148991	3.995473
786.672626	5441.114280	15.867341	-0.148980	3.992647
786.445551	5433.073354	15.872346	-0.148933	3.989785
785.944078	5425.165986	15.877351	-0.148834	3.986964
785.957640	5417.056287	15.882355	-0.148832	3.984078
786.163736	5409.117813	15.887360	-0.148865	3.981254
786.313999	5401.083325	15.892365	-0.148887	3.978392
786.120160	5393.052432	15.897370	-0.148846	3.975525
786.416311	5385.073265	15.902375	-0.148896	3.972681
785.887356	5377.113630	15.907379	-0.148792	3.969829
786.352790	5369.077500	15.912384	-0.148874	3.966964
786.166880	5361.086965	15.917389	-0.148834	3.964103
786.165269	5353.135252	15.922394	-0.148828	3.961256
785.867687	5345.148698	15.927399	-0.148768	3.958390
786.125145	5337.116729	15.932403	-0.148810	3.955515
785.999556	5329.122225	15.937408	-0.148782	3.952644
785.934065	5321.113261	15.942413	-0.148764	3.949768
785.768934	5313.128963	15.947418	-0.148728	3.946896
785.753319	5305.106719	15.952423	-0.148720	3.944011
785.656389	5297.157703	15.957427	-0.148697	3.941149
785.756315	5289.073845	15.962432	-0.148710	3.938240
785.923103	5281.123363	15.967437	-0.148736	3.935378
785.924318	5273.083047	15.972442	-0.148731	3.932479
785.799809	5265.109476	15.977447	-0.148702	3.929599
785.832428	5257.123503	15.982451	-0.148703	3.926716
785.401957	5249.140105	15.987456	-0.148618	3.923823
785.376405	5241.172373	15.992461	-0.148608	3.920940
785.091983	5233.168562	15.997466	-0.148550	3.918038
785.009115	5225.169088	16.002471	-0.148529	3.915139
785.082732	5217.116727	16.007475	-0.148537	3.912222
784.767152	5209.107672	16.012480	-0.148473	3.909310
784.802170	5201.200011	16.017485	-0.148475	3.906440
784.269269	5193.155065	16.022490	-0.148370	3.903507
784.654351	5185.112191	16.027495	-0.148437	3.900591
784.904508	5177.144870	16.032499	-0.148478	3.897696
785.035258	5169.086802	16.037504	-0.148497	3.894765
785.024126	5161.115907	16.042509	-0.148490	3.891860
784.967487	5153.092626	16.047514	-0.148474	3.888933
784.745903	5145.159454	16.052519	-0.148427	3.886034
784.943060	5137.095420	16.057523	-0.148459	3.883093
784.839373	5129.115887	16.062528	-0.148434	3.880174
784.939690	5121.159585	16.067533	-0.148448	3.877266
784.299201	5113.224511	16.072538	-0.148323	3.874349
784.502813	5105.067615	16.077543	-0.148356	3.871365
784.695809	5097.024766	16.082547	-0.148386	3.868420
784.787300	5089.030085	16.087552	-0.148398	3.865489
784.414176	5081.189298	16.092557	-0.148324	3.862603
784.098067	5073.151805	16.097562	-0.148259	3.859643
784.099297	5065.182033	16.102567	-0.148254	3.856712
784.224425	5057.158037	16.107571	-0.148272	3.853762
783.991686	5049.163418	16.112576	-0.148224	3.850813
784.623337	5041.108190	16.117581	-0.148336	3.847857
783.862616	5033.197738	16.122586	-0.148189	3.844924
783.765942	5025.265660	16.127591	-0.148166	3.841994
783.853104	5017.190775	16.132595	-0.148177	3.839012
784.015551	5009.193001	16.137600	-0.148202	3.836059
783.637293	5001.247190	16.142605	-0.148126	3.833111
783.720374	4993.185310	16.147610	-0.148137	3.830128
783.683028	4985.203936	16.152615	-0.148124	3.827169
783.785244	4977.154275	16.157619	-0.148138	3.824186
783.638454	4969.199178	16.162624	-0.148106	3.821231
783.986133	4961.183955	16.167629	-0.148165	3.818261
783.536945	4953.248680	16.172634	-0.148076	3.815302
783.428578	4945.273953	16.177639	-0.148051	3.812333
783.571160	4937.188594	16.182643	-0.148072	3.809326
783.397825	4929.227718	16.187648	-0.148035	3.806356
783.431289	4921.225012	16.192653	-0.148035	3.803372
783.223151	4913.222734	16.197658	-0.147991	3.800381
782.983140	4905.314804	16.202663	-0.147942	3.797423
782.903549	4897.247503	16.207667	-0.147921	3.794406
782.961359	4889.205186	16.212672	-0.147927	3.791398
782.970308	4881.230498	16.217677	-0.147923	3.788413
783.298428	4873.159696	16.222682	-0.147979	3.785397
782.989043	4865.236684	16.227687	-0.147916	3.782419
782.831119	4857.214457	16.232691	-0.147882	3.779405
783.036701	4849.228251	16.237696	-0.147915	3.776410
783.345693	4841.203001	16.242701	-0.147967	3.773401
782.854920	4833.232681	16.247706	-0.147870	3.770392
782.626819	4825.275296	16.252711	-0.147823	3.767391
782.294962	4817.305861	16.257715	-0.147756	3.764381
782.161734	4809.323304	16.262720	-0.147726	3.761368
782.093799	4801.339050	16.267725	-0.147708	3.758353
782.012487	4793.314139	16.272730	-0.147687	3.755320
782.224606	4785.286640	16.277735	-0.147722	3.752291
782.432209	4777.246843	16.282739	-0.147755	3.749255
782.635703	4769.228569	16.287744	-0.147788	3.746224
782.470161	4761.301573	16.292749	-0.147751	3.743216
782.017618	4753.292059	16.297754	-0.147662	3.740168
781.809984	4745.340461	16.302759	-0.147618	3.737146
781.815689	4737.319474	16.307763	-0.147614	3.734099
781.827662	4729.334193	16.312768	-0.147611	3.731064
781.298622	4721.398823	16.317773	-0.147507	3.728032
781.112514	4713.359767	16.322778	-0.147467	3.724967
781.497679	4705.353118	16.327783	-0.147534	3.721925
781.589947	4697.301271	16.332787	-0.147546	3.718856
781.431526	4689.375999	16.337792	-0.147511	3.715827
781.319156	4681.347277	16.342797	-0.147485	3.712757
781.163615	4673.302744	16.347802	-0.147450	3.709678
781.188105	4665.334016	16.352807	-0.147450	3.706629
781.101862	4657.370903	16.357811	-0.147428	3.703577
781.213404	4649.336342	16.362816	-0.147444	3.700501
780.811761	4641.394919	16.367821	-0.147364	3.697444
780.669412	4633.353797	16.372826	-0.147332	3.694354
780.953124	4625.350682	16.377831	-0.147380	3.691286
780.790386	4617.341414	16.382835	-0.147344	3.688201
780.784403	4609.306641	16.387840	-0.147338	3.685109
780.839229	4601.383135	16.392845	-0.147343	3.682058
780.479777	4593.378860	16.397850	-0.147271	3.678963
780.439756	4585.428062	16.402855	-0.147258	3.675894
780.840061	4577.332374	16.407859	-0.147327	3.672778
780.600686	4569.392181	16.412864	-0.147277	3.669702
780.522278	4561.405949	16.417869	-0.147258	3.666611
780.189379	4553.405020	16.422874	-0.147190	3.663505
780.376700	4545.426473	16.427879	-0.147220	3.660418
779.866854	4537.501212	16.432883	-0.147120	3.657331
779.803264	4529.443083	16.437888	-0.147103	3.654201
779.920082	4521.443005	16.442893	-0.147119	3.651097
779.876415	4513.396492	16.447898	-0.147106	3.647967
779.602901	4505.449713	16.452903	-0.147050	3.644867
779.761222	4497.463192	16.457907	-0.147074	3.641761
779.646323	4489.468708	16.462912	-0.147047	3.638641
780.127252	4481.436583	16.467917	-0.147131	3.635520
779.992011	4473.460425	16.472922	-0.147101	3.632402
780.113227	4465.416592	16.477927	-0.147118	3.629262
779.900686	4457.459675	16.482931	-0.147074	3.626143
780.094149	4449.387948	16.487936	-0.147104	3.622989
780.393570	4441.417654	16.492941	-0.147155	3.619874
780.184167	4433.477268	16.497946	-0.147111	3.616754
779.713562	4425.523362	16.502951	-0.147018	3.613619
779.722778	4417.532200	16.507955	-0.147014	3.610480
780.082504	4409.488130	16.512960	-0.147076	3.607327
779.682606	4401.527338	16.517965	-0.146996	3.604183
779.859279	4393.522129	16.522970	-0.147024	3.601034
779.847498	4385.542116	16.527975	-0.147016	3.597888
779.695916	4377.534071	16.532979	-0.146983	3.594724
779.581528	4369.558125	16.537984	-0.146956	3.591571
779.505915	4361.581700	16.542989	-0.146937	3.588416
779.045078	4353.591361	16.547994	-0.146846	3.585241
779.413147	4345.529129	16.552999	-0.146909	3.582059
779.175747	4337.593630	16.558003	-0.146860	3.578907
778.820614	4329.627428	16.563008	-0.146788	3.575737
779.082955	4321.562680	16.568013	-0.146832	3.572542
778.490889	4313.580389	16.573018	-0.146717	3.569353
778.971909	4305.552324	16.578023	-0.146801	3.566174
779.282304	4297.530486	16.583027	-0.146853	3.562989
778.980570	4289.577474	16.588032	-0.146792	3.559811
779.456025	4281.567727	16.593037	-0.146875	3.556631
778.923582	4273.616531	16.598042	-0.146771	3.553441
778.716083	4265.581294	16.603047	-0.146727	3.550225
778.772886	4257.602326	16.608051	-0.146732	3.547036
778.238654	4249.623414	16.613056	-0.146628	3.543826
778.084487	4241.680244	16.618061	-0.146594	3.540639
778.331400	4233.591865	16.623066	-0.146634	3.537403
778.430477	4225.570944	16.628071	-0.146647	3.534187
778.549425	4217.621029	16.633075	-0.146664	3.530997
778.264232	4209.612737	16.638080	-0.146606	3.527768
777.853721	4201.660234	16.643085	-0.146524	3.524555
778.350994	4193.644262	16.648090	-0.146612	3.521341
777.897902	4185.716702	16.653095	-0.146522	3.518131
777.647551	4177.753958	16.658099	-0.146470	3.514909
777.536050	4169.731548	16.663104	-0.146444	3.511665
777.718765	4161.676918	16.668109	-0.146473	3.508414
777.559654	4153.649188	16.673114	-0.146438	3.505160
777.013588	4145.817708	16.678119	-0.146331	3.501971
776.657189	4137.824164	16.683123	-0.146260	3.498719
777.179459	4129.687435	16.688128	-0.146352	3.495433
777.670622	4121.665798	16.693133	-0.146438	3.492190
777.334543	4113.690118	16.698138	-0.146370	3.488937
777.902505	4105.642588	16.703143	-0.146470	3.485680
777.414614	4097.762075	16.708147	-0.146374	3.482454
777.009144	4089.791509	16.713152	-0.146294	3.479192
776.676136	4081.866463	16.718157	-0.146226	3.475947
776.557721	4073.813546	16.723162	-0.146199	3.472653
777.007789	4065.721593	16.728167	-0.146278	3.469359
777.133812	4057.741489	16.733171	-0.146296	3.466097
776.813724	4049.732890	16.738176	-0.146231	3.462806
776.749012	4041.755740	16.743181	-0.146214	3.459533
776.200412	4033.914749	16.748186	-0.146106	3.456297
776.549730	4025.805511	16.753191	-0.146166	3.452977
776.994415	4017.739474	16.758195	-0.146244	3.449675
776.841482	4009.758106	16.763200	-0.146210	3.446384
776.821334	4001.818357	16.768205	-0.146201	3.443113
776.711915	3993.829864	16.773210	-0.146175	3.439814
776.598826	3985.872066	16.778215	-0.146149	3.436526
776.820760	3977.839453	16.783219	-0.146185	3.433214
776.711391	3969.821994	16.788224	-0.146159	3.429895
776.631099	3961.880067	16.793229	-0.146139	3.426604
776.510290	3953.897185	16.798234	-0.146112	3.423292
776.385075	3945.915682	16.803239	-0.146083	3.419977
776.518324	3937.892064	16.808243	-0.146103	3.416650
776.515133	3929.867982	16.813248	-0.146097	3.413315
776.579433	3921.902404	16.818253	-0.146103	3.410004
776.146122	3913.952227	16.823258	-0.146017	3.406678
776.169911	3905.944193	16.828263	-0.146017	3.403341
775.681485	3898.066858	16.833267	-0.145921	3.400037
775.657432	3890.015042	16.838272	-0.145911	3.396674
775.295989	3882.040612	16.843277	-0.145838	3.393327
775.422051	3873.944443	16.848282	-0.145856	3.389944
775.606271	3865.908755	16.853287	-0.145885	3.386584
775.609189	3857.950619	16.858291	-0.145881	3.383247
774.929659	3850.032174	16.863296	-0.145749	3.379899
775.244698	3842.030704	16.868301	-0.145802	3.376549
774.990134	3834.014315	16.873306	-0.145750	3.373168
775.036929	3825.975173	16.878311	-0.145753	3.369786
774.973814	3818.006064	16.883315	-0.145736	3.366425
774.976262	3809.987543	16.888320	-0.145731	3.363043
774.813181	3802.076303	16.893325	-0.145696	3.359696
774.914278	3794.061681	16.898330	-0.145709	3.356312
775.408740	3785.965824	16.903335	-0.145796	3.352905
775.064013	3778.050779	16.908339	-0.145727	3.349540
774.393087	3770.144176	16.913344	-0.145597	3.346163
774.605989	3762.132294	16.918349	-0.145631	3.342771
774.547759	3754.114607	16.923354	-0.145615	3.339363
774.338088	3746.191003	16.928359	-0.145571	3.335985
774.278617	3738.168558	16.933363	-0.145554	3.332568
774.601298	3730.079855	16.938368	-0.145609	3.329133
774.169352	3722.188568	16.943373	-0.145523	3.325751
774.422087	3714.143634	16.948378	-0.145565	3.322325
774.482892	3706.128934	16.953383	-0.145571	3.318901
774.303999	3698.199109	16.958387	-0.145533	3.315502
774.300483	3690.178180	16.963392	-0.145527	3.312066
774.420402	3682.190271	16.968397	-0.145544	3.308645
773.653056	3674.271410	16.973402	-0.145396	3.305217
773.327559	3666.296286	16.978407	-0.145330	3.301778
773.713218	3658.223220	16.983411	-0.145397	3.298320
774.005995	3650.160241	16.988416	-0.145446	3.294860
773.711965	3642.251700	16.993421	-0.145386	3.291440
774.206860	3634.151772	16.998426	-0.145473	3.287964
773.661188	3626.282648	17.003431	-0.145366	3.284544
773.754226	3618.325266	17.008435	-0.145378	3.281107
773.184901	3610.357621	17.013440	-0.145267	3.277636
773.592368	3602.296314	17.018445	-0.145337	3.274159
773.460991	3594.308957	17.023450	-0.145308	3.270689
773.799317	3586.241319	17.028455	-0.145365	3.267199
773.807878	3578.302725	17.033459	-0.145362	3.263749
773.857261	3570.317875	17.038464	-0.145366	3.260276
773.552792	3562.382583	17.043469	-0.145304	3.256807
773.574619	3554.351471	17.048474	-0.145303	3.253306
773.849344	3546.311407	17.053479	-0.145348	3.249807
773.633262	3538.393034	17.058483	-0.145303	3.246338
773.233929	3530.435289	17.063488	-0.145223	3.242840
773.072974	3522.440709	17.068493	-0.145188	3.239333
772.843882	3514.526679	17.073498	-0.145140	3.235853
772.846054	3506.497364	17.078503	-0.145135	3.232329
773.005252	3498.455052	17.083507	-0.145160	3.228802
772.700199	3490.447140	17.088512	-0.145098	3.225267
772.598904	3482.487877	17.093517	-0.145074	3.221758
773.236294	3474.395060	17.098522	-0.145187	3.218217
772.811484	3466.485750	17.103527	-0.145103	3.214708
772.913013	3458.497512	17.108531	-0.145116	3.211183
772.797748	3450.472877	17.113536	-0.145090	3.207629
773.306158	3442.403776	17.118541	-0.145179	3.204078
773.060675	3434.502195	17.123546	-0.145128	3.200565
772.819572	3426.547120	17.128551	-0.145078	3.197024
773.140379	3418.499684	17.133555	-0.145132	3.193463
772.635547	3410.593914	17.138560	-0.145033	3.189925
772.517868	3402.629996	17.143565	-0.145006	3.186374
772.458253	3394.588951	17.148570	-0.144990	3.182787
772.773832	3386.553130	17.153575	-0.145043	3.179215
772.997540	3378.567856	17.158579	-0.145080	3.175657
772.527271	3370.622771	17.163584	-0.144987	3.172083
772.599265	3362.629597	17.168589	-0.144995	3.168507
772.611282	3354.631732	17.173594	-0.144992	3.164923
772.276899	3346.740499	17.178599	-0.144925	3.161367
772.329933	3338.730368	17.183603	-0.144929	3.157770
771.906512	3330.753553	17.188608	-0.144845	3.154164
772.369078	3322.698906	17.193613	-0.144926	3.150557
771.765675	3314.781730	17.198618	-0.144808	3.146961
771.421972	3306.798687	17.203623	-0.144739	3.143342
771.488007	3298.786849	17.208627	-0.144746	3.139725
771.520514	3290.773030	17.213632	-0.144747	3.136101
771.476980	3282.793180	17.218637	-0.144734	3.132485
771.622686	3274.743324	17.223642	-0.144755	3.128841
771.394216	3266.786543	17.228647	-0.144708	3.125219
771.934506	3258.740904	17.233651	-0.144803	3.121586
771.470212	3250.854917	17.238656	-0.144711	3.117977
771.481839	3242.848729	17.243661	-0.144708	3.114330
771.468679	3234.888594	17.248666	-0.144701	3.110699
771.290368	3226.882521	17.253671	-0.144662	3.107035
771.328549	3218.879322	17.258675	-0.144664	3.103378
770.921124	3210.958196	17.263680	-0.144583	3.099733
770.903280	3203.004028	17.268685	-0.144574	3.096088
771.132870	3194.909868	17.273690	-0.144612	3.092385
770.775261	3186.947714	17.278695	-0.144540	3.088711
771.154988	3178.922704	17.283699	-0.144605	3.085038
771.273485	3170.922004	17.288704	-0.144622	3.081359
771.035280	3163.006936	17.293709	-0.144573	3.077699
771.146407	3154.986113	17.298714	-0.144588	3.074002
770.929121	3146.992814	17.303719	-0.144542	3.070299
771.012043	3138.991443	17.308723	-0.144553	3.066601
770.603443	3131.046585	17.313728	-0.144471	3.062901
770.668894	3123.081800	17.318733	-0.144478	3.059210
770.890949	3115.029887	17.323738	-0.144514	3.055482
770.489206	3107.102183	17.328743	-0.144434	3.051777
770.905670	3099.030289	17.333747	-0.144507	3.048040
770.538838	3091.098494	17.338752	-0.144433	3.044325
770.576469	3083.162816	17.343757	-0.144435	3.040624
769.947334	3075.277164	17.348762	-0.144313	3.036910
770.549206	3067.122264	17.353767	-0.144419	3.033124
770.565913	3059.146691	17.358771	-0.144417	3.029390
769.970876	3051.234718	17.363776	-0.144301	3.025650
769.917425	3043.288915	17.368781	-0.144286	3.021917
770.130271	3035.218248	17.373786	-0.144320	3.018134
769.980768	3027.230036	17.378791	-0.144287	3.014366
769.851449	3019.283535	17.383795	-0.144258	3.010615
769.730446	3011.281334	17.388800	-0.144230	3.006833
769.916950	3003.266765	17.393805	-0.144260	3.003056
769.515808	2995.361820	17.398810	-0.144180	2.999296
769.682162	2987.370744	17.403815	-0.144205	2.995519
769.564890	2979.410504	17.408819	-0.144178	2.991738
769.429913	2971.388681	17.413824	-0.144148	2.987922
769.129738	2963.439369	17.418829	-0.144087	2.984128
769.286037	2955.416957	17.423834	-0.144111	2.980316
769.359035	2947.421474	17.428839	-0.144119	2.976509
769.132015	2939.484608	17.433843	-0.144072	2.972709
769.003538	2931.461932	17.438848	-0.144042	2.968868
769.019170	2923.479228	17.443853	-0.144040	2.965049
768.890286	2915.528200	17.448858	-0.144011	2.961233
768.979755	2907.527555	17.453863	-0.144022	2.957399
768.973245	2899.538503	17.458867	-0.144016	2.953561
768.969205	2891.517412	17.463872	-0.144010	2.949702
768.688145	2883.600950	17.468877	-0.143952	2.945875
768.747577	2875.604291	17.473882	-0.143958	2.942021
768.672536	2867.599098	17.478887	-0.143939	2.938151
768.832339	2859.623444	17.483891	-0.143963	2.934303
769.226421	2851.554002	17.488896	-0.144031	2.930417
768.478648	2843.731792	17.493901	-0.143887	2.926585
768.767264	2835.675036	17.498906	-0.143935	2.922689
768.867455	2827.664933	17.503911	-0.143949	2.918801
768.754737	2819.765755	17.508915	-0.143923	2.914950
768.379484	2811.739537	17.513920	-0.143848	2.911017
768.444453	2803.718029	17.518925	-0.143854	2.907106
768.611298	2795.706246	17.523930	-0.143880	2.903199
768.186359	2787.789111	17.528935	-0.143796	2.899302
768.017698	2779.885010	17.533939	-0.143759	2.895419
767.885144	2771.859799	17.538944	-0.143729	2.891474
767.521708	2763.915733	17.543949	-0.143656	2.887551
767.470467	2755.907303	17.548954	-0.143642	2.883607
767.570144	2747.894279	17.553959	-0.143655	2.879664
767.315647	2740.008281	17.558963	-0.143602	2.875759
767.003380	2732.010784	17.563968	-0.143539	2.871791
767.483012	2723.900366	17.568973	-0.143623	2.867805
767.649456	2715.898498	17.573978	-0.143649	2.863849
767.339258	2707.998349	17.578983	-0.143586	2.859912
767.568092	2700.000740	17.583987	-0.143623	2.855952
767.821788	2691.965515	17.588992	-0.143665	2.851968
767.888326	2683.989481	17.593997	-0.143672	2.847999
767.464041	2676.080163	17.599002	-0.143588	2.844029
767.451202	2668.117921	17.604007	-0.143580	2.840050
767.355299	2660.175043	17.609011	-0.143557	2.836071
766.536957	2652.290173	17.614016	-0.143400	2.832073
767.354988	2644.113867	17.619021	-0.143547	2.828018
767.306648	2636.114932	17.624026	-0.143532	2.823996
766.986149	2628.208806	17.629031	-0.143468	2.820000
767.132380	2620.218427	17.634035	-0.143490	2.815982
766.850251	2612.278075	17.639040	-0.143432	2.811959
766.969991	2604.266566	17.644045	-0.143449	2.807918
766.767472	2596.305524	17.649050	-0.143406	2.803877
766.885512	2588.300585	17.654055	-0.143423	2.799827
767.222304	2580.326733	17.659059	-0.143480	2.795800
766.890012	2572.361907	17.664064	-0.143413	2.791733
767.107859	2564.344413	17.669069	-0.143448	2.787665
767.109223	2556.381415	17.674074	-0.143443	2.783606
767.020034	2548.406351	17.679079	-0.143421	2.779529
767.127008	2540.449446	17.684083	-0.143436	2.775468
766.707831	2532.502837	17.689088	-0.143353	2.771374
766.507481	2524.565714	17.694093	-0.143310	2.767293
766.276834	2516.617233	17.699098	-0.143262	2.763197
766.316034	2508.592564	17.704103	-0.143264	2.759073
766.159329	2500.670752	17.709107	-0.143230	2.754983
765.723409	2492.687234	17.714112	-0.143143	2.750839
765.406052	2484.706835	17.719117	-0.143079	2.746697
765.674031	2476.662836	17.724122	-0.143124	2.742551
765.642799	2468.686136	17.729127	-0.143113	2.738416
765.183107	2460.787939	17.734131	-0.143022	2.734289
765.187362	2452.762186	17.739136	-0.143017	2.730118
765.047719	2444.786189	17.744141	-0.142986	2.725958
765.074280	2436.794862	17.749146	-0.142986	2.721793
765.078664	2428.821980	17.754151	-0.142981	2.717631
765.061133	2420.883020	17.759155	-0.142973	2.713478
765.097113	2412.850339	17.764160	-0.142974	2.709274
765.065944	2404.855406	17.769165	-0.142963	2.705078
765.495837	2396.824035	17.774170	-0.143038	2.700886
765.212903	2388.919116	17.779175	-0.142980	2.696708
765.876858	2380.840858	17.784179	-0.143099	2.692493
765.461853	2372.944710	17.789184	-0.143016	2.688299
765.716633	2364.929390	17.794189	-0.143058	2.684078
765.477152	2357.079475	17.799194	-0.143009	2.679907
765.304794	2349.109064	17.804199	-0.142971	2.675669
765.111065	2341.151626	17.809203	-0.142930	2.671430
765.173410	2333.131202	17.814208	-0.142936	2.667167
765.233400	2325.139656	17.819213	-0.142942	2.662913
764.709853	2317.266561	17.824218	-0.142839	2.658677
764.705223	2309.249500	17.829223	-0.142833	2.654391
764.889084	2301.256387	17.834227	-0.142862	2.650123
764.677997	2293.288416	17.839232	-0.142818	2.645836
764.108137	2285.428659	17.844237	-0.142707	2.641577
764.514202	2277.363845	17.849242	-0.142777	2.637265
764.255226	2269.395094	17.854247	-0.142723	2.632953
764.455844	2261.390041	17.859251	-0.142755	2.628645
764.050229	2253.460817	17.864256	-0.142675	2.624331
763.967673	2245.506884	17.869261	-0.142654	2.620018
763.762054	2237.563241	17.874266	-0.142611	2.615695
763.765225	2229.548073	17.879271	-0.142606	2.611340
763.835386	2221.569744	17.884275	-0.142614	2.607002
763.731840	2213.595108	17.889280	-0.142589	2.602647
762.977115	2205.767972	17.894285	-0.142444	2.598321
763.839602	2197.599939	17.899290	-0.142599	2.593912
763.658667	2189.534895	17.904295	-0.142560	2.589480
763.443460	2181.621041	17.909299	-0.142515	2.585122
763.859482	2173.600549	17.914304	-0.142587	2.580741
763.574957	2165.701063	17.919309	-0.142529	2.576370
763.791599	2157.698592	17.924314	-0.142564	2.571971
763.940956	2149.713369	17.929319	-0.142586	2.567568
764.043347	2141.763459	17.934323	-0.142600	2.563174
763.217910	2133.944511	17.939328	-0.142441	2.558781
763.752605	2125.865769	17.944333	-0.142536	2.554330
763.576181	2117.949326	17.949338	-0.142498	2.549913
763.282329	2109.989724	17.954343	-0.142438	2.545455
763.596076	2101.983368	17.959347	-0.142491	2.541007
763.874670	2093.975523	17.964352	-0.142537	2.536547
763.834100	2086.032080	17.969357	-0.142525	2.532093
763.473619	2078.111873	17.974362	-0.142452	2.527621
763.070016	2070.206706	17.979367	-0.142372	2.523146
763.443071	2062.201786	17.984371	-0.142436	2.518663
763.167054	2054.251431	17.989376	-0.142379	2.514157
763.180254	2046.274976	17.994381	-0.142377	2.509648
762.601262	2038.389698	17.999386	-0.142264	2.505139
763.077582	2030.297303	18.004391	-0.142347	2.500582
762.998833	2022.378612	18.009395	-0.142327	2.496075
762.399136	2014.480627	18.014400	-0.142210	2.491533
762.473757	2006.455876	18.019405	-0.142219	2.486960
762.648352	1998.460410	18.024410	-0.142246	2.482403
762.512336	1990.525887	18.029415	-0.142216	2.477849
762.642932	1982.541682	18.034419	-0.142235	2.473278
762.381434	1974.620021	18.039424	-0.142181	2.468706
761.915045	1966.703933	18.044429	-0.142089	2.464112
762.015920	1958.723021	18.049434	-0.142102	2.459516
762.230555	1950.695110	18.054439	-0.142137	2.454892
762.173438	1942.733717	18.059443	-0.142121	2.450277
762.078727	1934.764603	18.064448	-0.142098	2.445646
761.853155	1926.878023	18.069453	-0.142051	2.441045
762.189169	1918.857207	18.074458	-0.142108	2.436399
762.334319	1910.816248	18.079463	-0.142130	2.431719
762.059921	1902.912534	18.084467	-0.142074	2.427077
762.065835	1894.936956	18.089472	-0.142070	2.422406
761.921714	1887.012579	18.094477	-0.142038	2.417744
762.189815	1878.993691	18.099482	-0.142082	2.413050
762.025306	1871.041376	18.104487	-0.142047	2.408352
762.097140	1863.094085	18.109491	-0.142055	2.403666
762.168800	1855.136684	18.114496	-0.142063	2.398965
761.972059	1847.216445	18.119501	-0.142021	2.394256
761.434596	1839.352208	18.124506	-0.141916	2.389544
761.478767	1831.344435	18.129511	-0.141919	2.384783
761.672331	1823.363713	18.134515	-0.141950	2.380041
761.323051	1815.431970	18.139520	-0.141879	2.375275
761.371751	1807.447480	18.144525	-0.141883	2.370499
761.222667	1799.519190	18.149530	-0.141850	2.365732
761.543364	1791.488089	18.154535	-0.141905	2.360932
761.533808	1783.575965	18.159539	-0.141898	2.356166
761.618740	1775.584368	18.164544	-0.141908	2.351351
761.462089	1767.647209	18.169549	-0.141874	2.346539
761.438660	1759.686738	18.174554	-0.141864	2.341713
761.333021	1751.741003	18.179559	-0.141839	2.336880
761.124705	1743.834446	18.184563	-0.141795	2.332053
761.247445	1735.818986	18.189568	-0.141813	2.327176
760.736850	1727.958177	18.194573	-0.141713	2.322331
760.931490	1719.969382	18.199578	-0.141744	2.317456
760.701001	1712.020586	18.204583	-0.141696	2.312560
760.581047	1704.077939	18.209587	-0.141668	2.307666
760.692690	1696.089311	18.214592	-0.141684	2.302753
760.803094	1688.140289	18.219597	-0.141699	2.297854
760.325050	1680.245988	18.224602	-0.141605	2.292929
759.581654	1672.385653	18.229607	-0.141461	2.287991
759.651307	1664.403024	18.234611	-0.141469	2.283036
760.079824	1656.360551	18.239616	-0.141543	2.278064
760.074722	1648.373331	18.244621	-0.141537	2.273078
760.226011	1640.375231	18.249626	-0.141560	2.268087
760.108327	1632.427700	18.254631	-0.141533	2.263095
759.693466	1624.565365	18.259635	-0.141451	2.258118
759.804411	1616.566519	18.264640	-0.141466	2.253091
760.054964	1608.576118	18.269645	-0.141507	2.248070
759.820919	1600.670239	18.274650	-0.141459	2.243048
759.399120	1592.784091	18.279655	-0.141375	2.238012
759.333570	1584.851666	18.284659	-0.141357	2.232966
759.456576	1576.850071	18.289664	-0.141375	2.227881
759.429877	1568.880801	18.294669	-0.141365	2.222792
759.474243	1560.937109	18.299674	-0.141368	2.217713
759.409589	1552.988236	18.304679	-0.141351	2.212611
759.095426	1545.098212	18.309683	-0.141287	2.207511
759.306117	1537.104435	18.314688	-0.141321	2.202380
759.397253	1529.166530	18.319693	-0.141333	2.197263
759.195458	1521.268229	18.324698	-0.141290	2.192133
758.910355	1513.323917	18.329703	-0.141232	2.186953
759.248275	1505.327285	18.334707	-0.141289	2.181784
758.694307	1497.463322	18.339712	-0.141181	2.176607
758.774504	1489.476969	18.344717	-0.141191	2.171396
758.955762	1481.509127	18.349722	-0.141219	2.166194
759.104651	1473.537818	18.354727	-0.141242	2.160975
758.739092	1465.676152	18.359731	-0.141168	2.155766
758.782535	1457.711685	18.364736	-0.141171	2.150516
758.592120	1449.795619	18.369741	-0.141131	2.145263
758.335793	1441.908514	18.374746	-0.141078	2.140010
758.105813	1433.963972	18.379751	-0.141030	2.134708
757.902806	1426.067501	18.384755	-0.140987	2.129427
757.564826	1418.140850	18.389760	-0.140919	2.124100
757.805118	1410.147943	18.394765	-0.140958	2.118771
757.754471	1402.209270	18.399770	-0.140943	2.113437
757.694930	1394.221751	18.404775	-0.140927	2.108056
757.307221	1386.356442	18.409779	-0.140850	2.102711
757.456663	1378.376871	18.414784	-0.140872	2.097328
757.434931	1370.410535	18.419789	-0.140863	2.091923
757.179924	1362.520458	18.424794	-0.140810	2.086533
756.814000	1354.613565	18.429799	-0.140737	2.081107
757.170108	1346.629895	18.434803	-0.140798	2.075685
757.198058	1338.675757	18.439808	-0.140798	2.070237
756.911914	1330.774550	18.444813	-0.140740	2.064780
756.915386	1322.852751	18.449818	-0.140735	2.059323
757.058666	1314.897372	18.454823	-0.140757	2.053842
757.345588	1306.905116	18.459827	-0.140805	2.048336
756.814901	1299.066277	18.464832	-0.140701	2.042838
756.701056	1291.159660	18.469837	-0.140674	2.037320
756.945634	1283.199657	18.474842	-0.140715	2.031788
756.006317	1275.387324	18.479847	-0.140535	2.026221
756.603378	1267.334431	18.484851	-0.140641	2.020629
756.731850	1259.373029	18.489856	-0.140659	2.015037
756.440487	1251.495951	18.494861	-0.140600	2.009446
756.039113	1243.642333	18.499866	-0.140520	2.003844
755.857888	1235.720122	18.504871	-0.140481	1.998200
755.899478	1227.791248	18.509875	-0.140484	1.992559
755.455100	1219.903788	18.514880	-0.140396	1.986881
755.613333	1211.927679	18.519885	-0.140420	1.981186
755.558004	1204.024213	18.524890	-0.140404	1.975505
755.333531	1196.093007	18.529895	-0.140357	1.969769
755.027448	1188.229848	18.534899	-0.140295	1.964056
754.832111	1180.327589	18.539904	-0.140254	1.958311
754.841476	1172.384066	18.544909	-0.140250	1.952540
754.871195	1164.418364	18.549914	-0.140250	1.946739
754.857366	1156.469674	18.554919	-0.140243	1.940928
754.807152	1148.571933	18.559923	-0.140228	1.935133
754.391642	1140.700122	18.564928	-0.140146	1.929299
753.916462	1132.840730	18.569933	-0.140052	1.923450
754.006803	1124.905428	18.574938	-0.140064	1.917590
753.850446	1116.974039	18.579943	-0.140029	1.911687
753.731724	1109.053799	18.584947	-0.140002	1.905778
753.459174	1101.175882	18.589952	-0.139946	1.899865
753.558953	1093.223702	18.594957	-0.139959	1.893921
753.671636	1085.267440	18.599962	-0.139975	1.887955
753.565942	1077.352272	18.604967	-0.139950	1.881977
753.200041	1069.528765	18.609971	-0.139877	1.876020
753.102641	1061.594492	18.614976	-0.139854	1.869990
752.713263	1053.726789	18.619981	-0.139776	1.863957
752.729334	1045.813233	18.624986	-0.139774	1.857917
752.473276	1037.909061	18.629991	-0.139721	1.851833
752.151172	1030.027395	18.634995	-0.139656	1.845738
752.063233	1022.114624	18.640000	-0.139634	1.839626
751.836355	1014.241696	18.645005	-0.139587	1.833508
751.398528	1006.383919	18.650010	-0.139500	1.827357
750.838526	998.522170	18.655015	-0.139391	1.821166
750.852951	990.584997	18.660019	-0.139388	1.814965
750.253215	982.742984	18.665024	-0.139271	1.808742
749.521633	974.920746	18.670029	-0.139130	1.802498
749.102429	967.041538	18.675034	-0.139047	1.796224
747.917756	959.239138	18.680039	-0.138821	1.789896
747.324604	951.342368	18.685043	-0.138705	1.783542
746.342520	943.518138	18.690048	-0.138517	1.777175
745.718029	935.608401	18.695053	-0.138396	1.770761
745.007953	927.734428	18.700058	-0.138258	1.764342
744.205947	919.882849	18.705063	-0.138104	1.757905
743.545034	912.019647	18.710067	-0.137976	1.751453
742.834386	904.129578	18.715072	-0.137838	1.744949
742.225495	896.253623	18.720077	-0.137720	1.738444
742.038881	888.314234	18.725082	-0.137680	1.731917
741.311011	880.449362	18.730087	-0.137539	1.725357
740.055292	872.720539	18.735091	-0.137300	1.718816
739.421240	864.832851	18.740096	-0.137177	1.712198
739.291370	856.848979	18.745101	-0.137147	1.705541
738.969215	848.936965	18.750106	-0.137082	1.698892
738.419921	841.054915	18.755111	-0.136975	1.692212
738.247148	833.128060	18.760115	-0.136937	1.685518
736.904641	825.434720	18.765120	-0.136682	1.678838
736.363222	817.548174	18.770125	-0.136576	1.672074
735.843041	809.671456	18.775130	-0.136474	1.665294
735.136616	801.832132	18.780135	-0.136338	1.658493
735.117852	793.871356	18.785139	-0.136329	1.651654
734.909722	785.956351	18.790144	-0.136285	1.644799
734.683148	778.086610	18.795149	-0.136238	1.637952
734.244572	770.218440	18.800154	-0.136151	1.631049
733.433809	762.398752	18.805159	-0.135995	1.624106
732.955622	754.574947	18.810163	-0.135901	1.617176
732.388849	746.731602	18.815168	-0.135790	1.610186
731.679679	738.928109	18.820173	-0.135653	1.603181
731.516122	731.033157	18.825178	-0.135617	1.596142
730.801809	723.231935	18.830183	-0.135479	1.589076
730.472011	715.362822	18.835187	-0.135412	1.581972
729.633114	707.587430	18.840192	-0.135251	1.574847
729.045413	699.764992	18.845197	-0.135136	1.567684
728.318731	691.979943	18.850202	-0.134996	1.560500
727.459846	684.196428	18.855207	-0.134831	1.553266
727.142552	676.302873	18.860211	-0.134767	1.545976
726.948135	668.407287	18.865216	-0.134725	1.538669
726.644234	660.534516	18.870221	-0.134664	1.531331
726.202686	652.721799	18.875226	-0.134576	1.523993
725.628242	644.929314	18.880231	-0.134464	1.516618
725.356258	637.084244	18.885235	-0.134408	1.509203
724.940215	629.260250	18.890240	-0.134326	1.501750
724.058414	621.542104	18.895245	-0.134157	1.494287
723.713458	613.692222	18.900250	-0.134087	1.486745
723.474910	605.845409	18.905255	-0.134038	1.479184
723.438180	597.972525	18.910259	-0.134026	1.471590
722.739926	590.194034	18.915264	-0.133890	1.463944
721.931313	582.463732	18.920269	-0.133735	1.456286
721.833232	574.604296	18.925274	-0.133711	1.448576
721.351733	566.828541	18.930279	-0.133617	1.440844
720.809603	559.070251	18.935283	-0.133511	1.433078
719.901483	551.356521	18.940288	-0.133336	1.425254
719.827942	543.506972	18.945293	-0.133318	1.417388
719.173167	535.776297	18.950298	-0.133191	1.409502
718.711822	527.990949	18.955303	-0.133100	1.401547
718.617912	520.182125	18.960307	-0.133077	1.393585
717.867514	512.451229	18.965312	-0.132932	1.385546
717.319279	504.700705	18.970317	-0.132825	1.377474
716.733075	496.974584	18.975322	-0.132711	1.369372
716.464318	489.165733	18.980327	-0.132656	1.361191
716.094191	481.411910	18.985331	-0.132582	1.353001
715.719534	473.634577	18.990336	-0.132507	1.344735
715.424993	465.887201	18.995341	-0.132447	1.336464
715.147167	458.124535	19.000346	-0.132390	1.328127
714.273636	450.468554	19.005351	-0.132222	1.319746
713.864947	442.699025	19.010355	-0.132141	1.311271
713.437838	434.922910	19.015360	-0.132056	1.302731
712.712465	427.242732	19.020365	-0.131916	1.294185
712.134532	419.548870	19.025370	-0.131804	1.285594
711.959135	411.787835	19.030375	-0.131766	1.276945
711.409233	404.109400	19.035379	-0.131658	1.268260
711.150733	396.379074	19.040384	-0.131605	1.259511
710.615871	388.699932	19.045389	-0.131501	1.250706
709.995045	381.060148	19.050394	-0.131380	1.241866
709.370332	373.408340	19.055399	-0.131259	1.232949
709.108601	365.687818	19.060403	-0.131205	1.223957
708.375772	358.072144	19.065408	-0.131063	1.214929
707.347445	350.495646	19.070413	-0.130867	1.205819
707.200906	342.783287	19.075418	-0.130835	1.196656
706.959621	335.074820	19.080423	-0.130785	1.187408
706.364084	327.455422	19.085427	-0.130669	1.178122
705.928723	319.806156	19.090432	-0.130583	1.168758
705.026642	312.268236	19.095437	-0.130410	1.159358
704.266467	304.696186	19.100442	-0.130263	1.149868
703.888295	297.024979	19.105447	-0.130188	1.140256
703.327864	289.420606	19.110451	-0.130078	1.130608
703.040982	281.775064	19.115456	-0.130020	1.120883
702.203037	274.251553	19.120461	-0.129859	1.111108
701.574370	266.696300	19.125466	-0.129737	1.101252
701.742914	258.992741	19.130471	-0.129763	1.091292
701.350316	251.431461	19.135475	-0.129685	1.081300
700.234736	244.023290	19.140480	-0.129473	1.071252
699.551224	236.493925	19.145485	-0.129340	1.061046
699.148914	228.952815	19.150490	-0.129260	1.050791
698.682089	221.416024	19.155495	-0.129169	1.040425
698.234152	213.901825	19.160499	-0.129080	1.029990
697.848641	206.396220	19.165504	-0.129004	1.019475
697.386961	198.901351	19.170509	-0.128913	1.008847
696.866896	191.455795	19.175514	-0.128811	0.998162
696.195776	184.008729	19.180519	-0.128681	0.987320
695.520331	176.599698	19.185523	-0.128550	0.976412
694.401748	169.271186	19.190528	-0.128337	0.965385
694.233079	161.773850	19.195533	-0.128301	0.954225
693.591458	154.401664	19.200538	-0.128177	0.942998
692.315750	147.144497	19.205543	-0.127934	0.931641
691.366476	139.841531	19.210547	-0.127753	0.920160
689.261441	132.761653	19.215552	-0.127356	0.908566
686.211678	125.806436	19.220557	-0.126784	0.896756
677.565951	119.809314	19.225562	-0.125170	0.884744
659.715970	115.247276	19.230567	-0.121843	0.872260
633.760766	111.803520	19.235571	-0.117008	0.859070
612.534565	107.208537	19.240576	-0.113053	0.845122
605.543828	100.001845	19.245581	-0.111746	0.830758
604.607833	91.839098	19.250586	-0.111567	0.816336
599.775484	84.509027	19.255591	-0.110662	0.801908
589.052213	78.471660	19.260595	-0.108662	0.787663