Mon Apr 19 09:09:08 2021

Number of Points = 3648
Depth (nm)	Load (N)	Time (s)	Depth (V)	Load (V)
0.962355	-0.141962	0.000000	-0.000200	0.310794

1.162091	-0.178845	0.005005	-0.000237	0.310791
1.448451	-0.232308	0.010010	-0.000291	0.310784
1.107989	-0.167824	0.015014	-0.000227	0.310796
1.186413	-0.182373	0.020019	-0.000242	0.310794
1.152575	-0.222075	0.025024	-0.000235	0.310580
0.891733	-0.179086	0.030029	-0.000187	0.310560
1.139269	-0.225931	0.035034	-0.000233	0.310551
0.820851	-0.168264	0.040038	-0.000174	0.310550
0.744469	-0.148995	0.045043	-0.000159	0.310575
0.784740	-0.160893	0.050048	-0.000167	0.310553
0.883462	-0.177438	0.055053	-0.000185	0.310560
0.936620	-0.229880	0.060058	-0.000195	0.310360
1.066128	-0.288297	0.065062	-0.000219	0.310197
0.589869	-0.198115	0.070067	-0.000130	0.310214
0.858764	-0.250587	0.075072	-0.000180	0.310197
0.864137	-0.248873	0.080077	-0.000181	0.310209
0.923551	-0.271794	0.085082	-0.000192	0.310153
1.021972	-0.346340	0.090086	-0.000210	0.309888
0.833707	-0.309129	0.095091	-0.000175	0.309902
0.768641	-0.298598	0.100096	-0.000163	0.309896
0.502088	-0.246503	0.105101	-0.000114	0.309913
0.611122	-0.317858	0.110106	-0.000134	0.309672
0.354434	-0.292392	0.115110	-0.000086	0.309573
0.337377	-0.287564	0.120115	-0.000083	0.309580
0.505455	-0.321616	0.125120	-0.000114	0.309564
1.121234	-0.463310	0.130125	-0.000229	0.309424
0.818158	-0.440387	0.135130	-0.000172	0.309274
0.787083	-0.435003	0.140134	-0.000166	0.309272
0.650130	-0.409952	0.145139	-0.000141	0.309273
0.607668	-0.472950	0.150144	-0.000133	0.308942
0.459727	-0.442799	0.155149	-0.000105	0.308957
0.590173	-0.467907	0.160154	-0.000129	0.308950
0.915593	-0.580899	0.165158	-0.000190	0.308698
0.927613	-0.597773	0.170163	-0.000192	0.308629
0.668568	-0.549753	0.175168	-0.000144	0.308633
0.397645	-0.553249	0.180173	-0.000093	0.308386
0.783053	-0.640121	0.185178	-0.000165	0.308306
0.815147	-0.649336	0.190182	-0.000171	0.308290
0.948044	-0.731048	0.195187	-0.000196	0.308020
1.021307	-0.747354	0.200192	-0.000209	0.308006
1.165623	-0.811278	0.205197	-0.000236	0.307828
0.963392	-0.809082	0.210202	-0.000198	0.307666
1.241725	-0.874710	0.215206	-0.000250	0.307595
1.341541	-0.945619	0.220211	-0.000269	0.307346
1.333010	-0.947741	0.225216	-0.000267	0.307329
1.229342	-0.993802	0.230221	-0.000248	0.307023
1.019901	-0.958305	0.235226	-0.000209	0.307011
0.906342	-0.989006	0.240230	-0.000187	0.306768
0.807308	-0.976091	0.245235	-0.000169	0.306744
0.914671	-1.049238	0.250240	-0.000189	0.306491
0.722001	-1.031678	0.255245	-0.000153	0.306409
0.841244	-1.093524	0.260250	-0.000175	0.306219
0.653763	-1.083993	0.265254	-0.000140	0.306102
0.721524	-1.133795	0.270259	-0.000153	0.305925
0.665167	-1.156322	0.275264	-0.000142	0.305770
0.400306	-1.134491	0.280269	-0.000093	0.305645
0.580726	-1.191722	0.285274	-0.000126	0.305529
0.726359	-1.266978	0.290278	-0.000153	0.305298
1.057211	-1.354611	0.295283	-0.000215	0.305167
0.573154	-1.319399	0.300288	-0.000125	0.304917
0.213809	-1.264196	0.305293	-0.000058	0.304869
0.310637	-1.345670	0.310298	-0.000076	0.304565
0.132447	-1.323993	0.315302	-0.000042	0.304514
0.257526	-1.400872	0.320307	-0.000066	0.304257
0.314908	-1.432484	0.325312	-0.000076	0.304156
0.465161	-1.512218	0.330317	-0.000104	0.303906
0.380816	-1.528782	0.335322	-0.000088	0.303754
0.183320	-1.524728	0.340326	-0.000052	0.303602
0.013678	-1.544436	0.345331	-0.000020	0.303361
-0.078278	-1.546055	0.350336	-0.000003	0.303274
0.346018	-1.682501	0.355341	-0.000082	0.302990
-0.137055	-1.619695	0.360346	0.000008	0.302871
0.066135	-1.703941	0.365350	-0.000029	0.302644
0.400277	-1.812586	0.370355	-0.000092	0.302415
0.207145	-1.809085	0.375360	-0.000056	0.302264
-0.261437	-1.777197	0.380365	0.000032	0.302008
-0.898448	-1.689231	0.385370	0.000150	0.301875
-0.433211	-1.804998	0.390374	0.000064	0.301725
-0.437357	-1.864386	0.395379	0.000065	0.301436
-0.651498	-1.855841	0.400384	0.000105	0.301291
-0.304202	-1.963241	0.405389	0.000040	0.301078
-0.334426	-2.006506	0.410394	0.000046	0.300843
-0.426429	-2.018824	0.415398	0.000063	0.300703
-0.528596	-2.035439	0.420403	0.000082	0.300534
-0.632865	-2.068650	0.425408	0.000101	0.300282
-0.352950	-2.155867	0.430413	0.000049	0.300107
-0.582926	-2.164642	0.435418	0.000092	0.299863
-1.138144	-2.112849	0.440422	0.000196	0.299626
-0.723472	-2.220406	0.445427	0.000119	0.299470
-1.070110	-2.202730	0.450432	0.000183	0.299251
-1.199027	-2.235649	0.455437	0.000207	0.298978
-0.650312	-2.372822	0.460442	0.000105	0.298796
-1.328677	-2.288628	0.465446	0.000231	0.298607
-1.232735	-2.367981	0.470451	0.000214	0.298307
-1.253632	-2.399883	0.475456	0.000218	0.298133
-1.422818	-2.404191	0.480461	0.000249	0.297963
-2.289238	-2.307865	0.485466	0.000410	0.297666
-2.514762	-2.304738	0.490470	0.000452	0.297481
-2.136227	-2.405909	0.495475	0.000382	0.297324
-2.813905	-2.345759	0.500480	0.000508	0.297017
-3.245132	-2.292250	0.505485	0.000589	0.296895
-3.284539	-2.316743	0.510490	0.000596	0.296741
-3.348631	-2.371225	0.515494	0.000608	0.296418
-3.804974	-2.308680	0.520499	0.000693	0.296318
-3.842900	-2.348519	0.525504	0.000700	0.296090
-3.922811	-2.379926	0.530509	0.000715	0.295865
-4.447075	-2.303879	0.535514	0.000813	0.295771
-4.415651	-2.359217	0.540518	0.000807	0.295528
-4.565326	-2.355837	0.545523	0.000835	0.295411
-5.782197	-2.174712	0.550528	0.001061	0.295214
-5.408019	-2.282783	0.555533	0.000992	0.295018
-5.449615	-2.302922	0.560538	0.001000	0.294882
-6.046131	-2.250395	0.565542	0.001111	0.294607
-5.169829	-2.429630	0.570547	0.000948	0.294509
-5.518571	-2.420826	0.575552	0.001013	0.294240
-6.065957	-2.344273	0.580557	0.001114	0.294127
-6.559650	-2.297434	0.585562	0.001206	0.293916
-6.385108	-2.364983	0.590566	0.001174	0.293739
-6.540975	-2.362670	0.595571	0.001203	0.293611
-7.440977	-2.248997	0.600576	0.001371	0.293365
-7.410554	-2.269147	0.605581	0.001365	0.293292
-7.037841	-2.385446	0.610586	0.001296	0.293053
-7.350234	-2.340722	0.615590	0.001354	0.292993
-7.912096	-2.299294	0.620595	0.001458	0.292693
-8.076305	-2.274972	0.625600	0.001489	0.292665
-8.355645	-2.283799	0.630605	0.001541	0.292370
-8.712555	-2.218770	0.635610	0.001608	0.292371
-9.065437	-2.215531	0.640614	0.001673	0.292069
-8.966810	-2.236582	0.645619	0.001655	0.292053
-10.081818	-2.080757	0.650624	0.001863	0.291821
-9.645294	-2.170377	0.655629	0.001781	0.291770
-9.377064	-2.257571	0.660634	0.001732	0.291579
-10.016793	-2.173109	0.665638	0.001851	0.291421
-10.291442	-2.141422	0.670643	0.001902	0.291330
-10.389942	-2.166782	0.675648	0.001920	0.291115
-9.994050	-2.247610	0.680653	0.001847	0.291070
-10.801310	-2.152355	0.685658	0.001997	0.290814
-10.640815	-2.184993	0.690662	0.001967	0.290797
-10.228325	-2.303439	0.695667	0.001890	0.290580
-10.877106	-2.194863	0.700672	0.002011	0.290533
-10.838272	-2.247217	0.705677	0.002004	0.290307
-10.758378	-2.284839	0.710682	0.001989	0.290192
-11.069698	-2.262156	0.715686	0.002047	0.290023
-11.732984	-2.167314	0.720691	0.002171	0.289894
-11.661894	-2.195292	0.725696	0.002157	0.289819
-11.207563	-2.334996	0.730701	0.002073	0.289533
-11.556713	-2.271522	0.735706	0.002138	0.289533
-11.571722	-2.328035	0.740710	0.002141	0.289236
-11.358847	-2.363290	0.745715	0.002101	0.289253
-12.361640	-2.244876	0.750720	0.002288	0.288934
-12.325544	-2.254317	0.755725	0.002281	0.288919
-12.465044	-2.266879	0.760730	0.002307	0.288729
-12.420578	-2.302191	0.765734	0.002299	0.288592
-12.393961	-2.333518	0.770739	0.002294	0.288459
-13.313941	-2.200386	0.775744	0.002465	0.288288
-12.499264	-2.361054	0.780749	0.002314	0.288224
-13.147620	-2.291463	0.785754	0.002435	0.287982
-13.471376	-2.231814	0.790758	0.002495	0.287985
-13.262790	-2.327348	0.795763	0.002456	0.287695
-13.484035	-2.298801	0.800768	0.002497	0.287637
-13.636604	-2.306829	0.805773	0.002526	0.287456
-14.322050	-2.203637	0.810778	0.002653	0.287348
-14.613213	-2.159924	0.815782	0.002708	0.287302
-14.656878	-2.206501	0.820787	0.002716	0.287027
-14.650411	-2.210378	0.825792	0.002715	0.287013
-14.783891	-2.219597	0.830797	0.002740	0.286844
-15.682160	-2.074917	0.835802	0.002907	0.286750
-15.454901	-2.117992	0.840806	0.002865	0.286741
-15.290773	-2.209796	0.845811	0.002834	0.286427
-15.776764	-2.125504	0.850816	0.002925	0.286407
-16.106504	-2.085419	0.855821	0.002986	0.286306
-15.848181	-2.173098	0.860826	0.002938	0.286100
-15.952324	-2.154558	0.865830	0.002957	0.286098
-15.845558	-2.218138	0.870835	0.002938	0.285874
-16.441363	-2.129081	0.875840	0.003049	0.285776
-16.139594	-2.187608	0.880845	0.002992	0.285758
-16.209966	-2.223653	0.885850	0.003006	0.285510
-16.474319	-2.175034	0.890854	0.003055	0.285513
-16.049331	-2.290155	0.895859	0.002976	0.285320
-16.742757	-2.193849	0.900864	0.003105	0.285169
-16.416418	-2.264382	0.905869	0.003044	0.285112
-16.666774	-2.270082	0.910874	0.003091	0.284852
-16.852547	-2.237463	0.915878	0.003125	0.284846
-17.117162	-2.233765	0.920883	0.003175	0.284620
-17.308607	-2.218247	0.925888	0.003210	0.284521
-16.812430	-2.324420	0.930893	0.003118	0.284440
-17.957389	-2.151830	0.935898	0.003331	0.284259
-17.878662	-2.168408	0.940902	0.003317	0.284247
-18.001315	-2.185119	0.945907	0.003340	0.284048
-18.119437	-2.192201	0.950912	0.003362	0.283902
-18.077051	-2.202081	0.955917	0.003354	0.283891
-18.588678	-2.162365	0.960922	0.003449	0.283619
-19.143017	-2.060300	0.965926	0.003552	0.283625
-19.331462	-2.037285	0.970931	0.003587	0.283568
-19.436372	-2.070999	0.975936	0.003607	0.283298
-18.978640	-2.155005	0.980941	0.003522	0.283294
-19.073671	-2.163289	0.985946	0.003540	0.283163
-19.657922	-2.090897	0.990950	0.003648	0.282990
-19.213036	-2.168909	0.995955	0.003566	0.283004
-19.215128	-2.220164	1.000960	0.003566	0.282740
-20.110158	-2.072761	1.005965	0.003733	0.282661
-19.648292	-2.157305	1.010970	0.003647	0.282658
-19.666655	-2.217299	1.015974	0.003650	0.282333
-19.621295	-2.225519	1.020979	0.003642	0.282333
-19.911055	-2.202524	1.025984	0.003696	0.282181
-20.158497	-2.189617	1.030989	0.003742	0.282016
-19.479820	-2.315308	1.035994	0.003616	0.282004
-20.481893	-2.187662	1.040998	0.003802	0.281724
-20.483526	-2.186449	1.046003	0.003803	0.281728
-20.629882	-2.182623	1.051008	0.003830	0.281611
-20.590141	-2.233862	1.056013	0.003823	0.281384
-20.751135	-2.202222	1.061018	0.003853	0.281396
-21.115193	-2.185096	1.066022	0.003920	0.281144
-21.469836	-2.129559	1.071027	0.003986	0.281097
-21.768468	-2.075751	1.076032	0.004042	0.281095
-21.722764	-2.142957	1.081037	0.004034	0.280791
-21.392377	-2.206077	1.086042	0.003972	0.280775
-22.406035	-2.031763	1.091046	0.004161	0.280723
-22.170064	-2.106993	1.096051	0.004117	0.280556
-21.599567	-2.215733	1.101056	0.004011	0.280530
-22.135320	-2.154281	1.106061	0.004111	0.280344
-22.987890	-2.025389	1.111066	0.004269	0.280209
-22.162911	-2.178541	1.116070	0.004116	0.280193
-22.131572	-2.232177	1.121075	0.004110	0.279945
-23.297528	-2.031792	1.126080	0.004327	0.279885
-22.559280	-2.173186	1.131085	0.004190	0.279847
-22.885407	-2.169743	1.136090	0.004250	0.279558
-23.389095	-2.079892	1.141094	0.004344	0.279549
-23.172510	-2.134687	1.146099	0.004304	0.279469
-23.198414	-2.171559	1.151104	0.004309	0.279253
-23.912919	-2.035173	1.156109	0.004442	0.279287
-23.957780	-2.062002	1.161114	0.004450	0.279105
-23.969320	-2.093318	1.166118	0.004452	0.278931
-23.234769	-2.228345	1.171123	0.004316	0.278924
-23.974144	-2.145872	1.176128	0.004454	0.278654
-24.388421	-2.077176	1.181133	0.004531	0.278619
-23.714518	-2.210655	1.186138	0.004405	0.278562
-24.493387	-2.122507	1.191142	0.004550	0.278284
-24.086899	-2.197232	1.196147	0.004475	0.278279
-24.061665	-2.230102	1.201152	0.004470	0.278132
-24.086478	-2.254732	1.206157	0.004475	0.277980
-23.943585	-2.288339	1.211162	0.004448	0.277940
-24.555422	-2.235195	1.216166	0.004562	0.277637
-24.332105	-2.272761	1.221171	0.004521	0.277653
-24.831968	-2.224165	1.226176	0.004614	0.277432
-24.893864	-2.232279	1.231181	0.004625	0.277330
-25.184285	-2.181564	1.236186	0.004679	0.277319
-25.232609	-2.233025	1.241190	0.004688	0.277004
-25.069581	-2.261438	1.246195	0.004658	0.277011
-24.866829	-2.336608	1.251200	0.004620	0.276810
-25.701790	-2.201540	1.256205	0.004776	0.276722
-25.613869	-2.228849	1.261210	0.004760	0.276663
-26.050435	-2.203204	1.266214	0.004841	0.276381
-25.492496	-2.303635	1.271219	0.004737	0.276386
-26.025409	-2.247105	1.276224	0.004836	0.276175
-26.575181	-2.164378	1.281229	0.004939	0.276084
-26.231991	-2.232713	1.286234	0.004875	0.276053
-26.674058	-2.209076	1.291238	0.004957	0.275755
-26.965610	-2.151242	1.296243	0.005011	0.275780
-27.017607	-2.163960	1.301248	0.005021	0.275663
-27.338129	-2.128359	1.306253	0.005081	0.275544
-27.121064	-2.168909	1.311258	0.005041	0.275538
-26.827169	-2.277454	1.316262	0.004986	0.275248
-26.749728	-2.306603	1.321267	0.004972	0.275169
-27.490304	-2.189757	1.326272	0.005109	0.275075
-27.835719	-2.165916	1.331277	0.005174	0.274869
-27.782249	-2.172841	1.336282	0.005164	0.274884
-28.292926	-2.122091	1.341286	0.005259	0.274662
-28.675479	-2.071380	1.346291	0.005330	0.274562
-28.797854	-2.047929	1.351296	0.005353	0.274568
-28.363615	-2.171332	1.356301	0.005272	0.274334
-28.889609	-2.085804	1.361306	0.005370	0.274280
-28.799993	-2.105309	1.366310	0.005354	0.274263
-28.114933	-2.295708	1.371315	0.005226	0.273915
-28.619058	-2.204521	1.376320	0.005320	0.273912
-29.418693	-2.079685	1.381325	0.005469	0.273803
-29.154732	-2.161515	1.386330	0.005420	0.273624
-29.191290	-2.157801	1.391334	0.005427	0.273608
-29.124904	-2.217135	1.396339	0.005414	0.273358
-29.278135	-2.204557	1.401344	0.005443	0.273277
-29.256645	-2.219195	1.406349	0.005439	0.273220
-29.828530	-2.156427	1.411354	0.005545	0.273001
-30.275041	-2.073735	1.416358	0.005629	0.273008
-29.571533	-2.235662	1.421363	0.005498	0.272828
-30.045650	-2.182840	1.426368	0.005586	0.272650
-29.675309	-2.252160	1.431373	0.005517	0.272640
-29.577523	-2.328699	1.436378	0.005499	0.272327
-29.994344	-2.253537	1.441382	0.005577	0.272324
-29.931637	-2.300333	1.446387	0.005565	0.272135
-30.303373	-2.256455	1.451392	0.005634	0.272009
-30.130549	-2.299193	1.456397	0.005602	0.271948
-30.943167	-2.192685	1.461402	0.005753	0.271728
-30.790590	-2.223215	1.466406	0.005725	0.271713
-30.812780	-2.256573	1.471411	0.005729	0.271514
-31.086805	-2.230779	1.476416	0.005780	0.271385
-31.245508	-2.209875	1.481421	0.005810	0.271343
-31.027263	-2.297254	1.486426	0.005769	0.271088
-31.612085	-2.191177	1.491430	0.005878	0.271086
-31.596476	-2.230238	1.496435	0.005875	0.270892
-32.264023	-2.130715	1.501440	0.006000	0.270775
-31.566016	-2.262633	1.506445	0.005870	0.270748
-32.184417	-2.192211	1.511450	0.005985	0.270523
-32.473167	-2.139703	1.516454	0.006039	0.270523
-32.202420	-2.214216	1.521459	0.005988	0.270387
-32.447584	-2.209978	1.526464	0.006034	0.270171
-32.523638	-2.196431	1.531469	0.006048	0.270169
-32.360341	-2.277232	1.536474	0.006018	0.269895
-32.436962	-2.273954	1.541478	0.006032	0.269838
-32.670390	-2.256254	1.546483	0.006076	0.269705
-33.412809	-2.153826	1.551488	0.006214	0.269529
-33.017922	-2.226159	1.556493	0.006140	0.269526
-33.016901	-2.270326	1.561498	0.006140	0.269290
-33.526429	-2.188503	1.566502	0.006235	0.269231
-33.132639	-2.278762	1.571507	0.006162	0.269131
-33.745641	-2.208877	1.576512	0.006276	0.268907
-33.880741	-2.185686	1.581517	0.006301	0.268899
-33.488040	-2.299720	1.586522	0.006228	0.268669
-33.807937	-2.255645	1.591526	0.006288	0.268593
-34.320627	-2.175855	1.596531	0.006383	0.268520
-34.460531	-2.196755	1.601536	0.006409	0.268270
-34.636062	-2.161764	1.606541	0.006442	0.268286
-34.511017	-2.219569	1.611546	0.006419	0.268097
-34.915144	-2.167282	1.616550	0.006494	0.267982
-34.025620	-2.340576	1.621555	0.006329	0.267920
-34.368877	-2.332681	1.626560	0.006393	0.267625
-34.742610	-2.264783	1.631565	0.006462	0.267624
-34.838323	-2.289166	1.636570	0.006480	0.267397
-34.702152	-2.331517	1.641574	0.006455	0.267302
-34.742741	-2.345807	1.646579	0.006462	0.267184
-35.459165	-2.252445	1.651584	0.006596	0.266984
-35.270403	-2.284629	1.656589	0.006561	0.266995
-35.158880	-2.354138	1.661594	0.006540	0.266728
-36.148734	-2.177366	1.666598	0.006724	0.266710
-36.042705	-2.222939	1.671603	0.006705	0.266567
-36.145630	-2.238004	1.676608	0.006724	0.266383
-36.359954	-2.197714	1.681613	0.006764	0.266390
-36.854837	-2.155090	1.686618	0.006856	0.266132
-36.987249	-2.138250	1.691622	0.006881	0.266093
-36.983626	-2.145446	1.696627	0.006880	0.266057
-37.259796	-2.148801	1.701632	0.006931	0.265765
-36.842289	-2.226099	1.706637	0.006854	0.265757
-36.790333	-2.258807	1.711642	0.006844	0.265630
-37.493358	-2.155602	1.716646	0.006975	0.265495
-37.073404	-2.230500	1.721651	0.006897	0.265503
-37.254236	-2.258624	1.726656	0.006931	0.265170
-37.592164	-2.199500	1.731661	0.006994	0.265157
-37.869361	-2.171265	1.736666	0.007045	0.265036
-38.189466	-2.150079	1.741670	0.007105	0.264833
-37.521435	-2.269408	1.746675	0.006981	0.264845
-38.082365	-2.217338	1.751680	0.007085	0.264571
-38.238204	-2.200658	1.756685	0.007114	0.264507
-38.121109	-2.234210	1.761690	0.007092	0.264440
-38.289257	-2.244943	1.766694	0.007124	0.264213
-38.693448	-2.166859	1.771699	0.007199	0.264238
-38.456510	-2.254380	1.776704	0.007155	0.263994
-38.967741	-2.180164	1.781709	0.007250	0.263891
-38.875810	-2.204193	1.786714	0.007233	0.263851
-39.386715	-2.159522	1.791718	0.007328	0.263585
-38.840416	-2.259612	1.796723	0.007227	0.263581
-39.391336	-2.194984	1.801728	0.007329	0.263386
-39.797135	-2.144005	1.806733	0.007405	0.263260
-39.412359	-2.211289	1.811738	0.007333	0.263274
-39.784330	-2.199335	1.816742	0.007402	0.262968
-39.595322	-2.234554	1.821747	0.007367	0.262963
-39.685912	-2.244511	1.826752	0.007384	0.262817
-39.852841	-2.249759	1.831757	0.007415	0.262620
-39.471331	-2.323251	1.836762	0.007344	0.262598
-40.184987	-2.248073	1.841766	0.007477	0.262296
-40.367584	-2.209736	1.846771	0.007511	0.262324
-40.519378	-2.214834	1.851776	0.007540	0.262143
-40.779828	-2.195685	1.856781	0.007588	0.261987
-40.445474	-2.254567	1.861786	0.007526	0.261997
-41.581621	-2.097806	1.866790	0.007737	0.261721
-41.344140	-2.140324	1.871795	0.007693	0.261725
-40.946520	-2.233736	1.876800	0.007619	0.261608
-41.073892	-2.254967	1.881805	0.007643	0.261362
-41.283411	-2.215842	1.886810	0.007682	0.261367
-41.589145	-2.206319	1.891814	0.007739	0.261111
-41.792683	-2.175184	1.896819	0.007777	0.261078
-42.154824	-2.121818	1.901824	0.007844	0.261009
-42.685670	-2.070256	1.906829	0.007943	0.260759
-42.303620	-2.139013	1.911834	0.007872	0.260763
-41.941199	-2.228281	1.916838	0.007805	0.260633
-42.216080	-2.201130	1.921843	0.007856	0.260505
-42.161348	-2.212982	1.926848	0.007846	0.260495
-42.439525	-2.221143	1.931853	0.007898	0.260168
-42.624252	-2.188088	1.936858	0.007932	0.260164
-42.570767	-2.227326	1.941862	0.007922	0.260000
-42.829351	-2.208152	1.946867	0.007970	0.259844
-42.720556	-2.230206	1.951872	0.007950	0.259831
-43.415714	-2.160042	1.956877	0.008080	0.259517
-43.232433	-2.191609	1.961882	0.008046	0.259527
-43.239035	-2.215366	1.966886	0.008047	0.259387
-43.848922	-2.130884	1.971891	0.008160	0.259239
-43.917996	-2.118712	1.976896	0.008173	0.259237
-43.719441	-2.203729	1.981901	0.008136	0.258963
-43.849265	-2.192540	1.986906	0.008161	0.258894
-44.307681	-2.121731	1.991910	0.008246	0.258823
-43.850316	-2.246969	1.996915	0.008161	0.258587
-44.458092	-2.156151	2.001920	0.008274	0.258477

-44.354325	-2.213817	2.011917	0.008255	0.258259
-44.525376	-2.228515	2.021914	0.008287	0.258001
-44.908542	-2.176258	2.031910	0.008358	0.257903
-45.202634	-2.170050	2.041907	0.008413	0.257637
-44.968022	-2.229665	2.051904	0.008369	0.257541
-45.304114	-2.207706	2.061901	0.008432	0.257320
-45.388375	-2.192716	2.071898	0.008448	0.257318
-45.418085	-2.229058	2.081894	0.008454	0.257082
-45.672894	-2.198641	2.091891	0.008501	0.256992
-45.504369	-2.229520	2.101888	0.008470	0.256990
-45.901786	-2.154813	2.111885	0.008544	0.257003
-45.859876	-2.194861	2.121882	0.008536	0.256820
-45.802510	-2.225233	2.131878	0.008526	0.256707
-46.137255	-2.162824	2.141875	0.008588	0.256715
-46.226903	-2.147112	2.151872	0.008605	0.256712
-45.787691	-2.228499	2.161869	0.008523	0.256703
-45.951881	-2.196815	2.171866	0.008554	0.256713
-45.980269	-2.190843	2.181862	0.008559	0.256717
-46.302131	-2.131415	2.191859	0.008619	0.256721
-46.330639	-2.083871	2.201856	0.008624	0.256960
-45.558750	-2.219004	2.211853	0.008481	0.256989
-45.978406	-2.140192	2.221850	0.008559	0.257002
-45.571076	-2.214854	2.231846	0.008483	0.256999
-45.954307	-2.144337	2.241843	0.008555	0.257003
-45.858453	-2.127598	2.251840	0.008537	0.257195
-45.287418	-2.209307	2.261837	0.008431	0.257320
-45.609816	-2.148260	2.271834	0.008491	0.257333
-45.246205	-2.216488	2.281830	0.008423	0.257320
-45.051543	-2.197837	2.291827	0.008387	0.257624
-45.062553	-2.193634	2.301824	0.008389	0.257636
-44.637496	-2.272328	2.311821	0.008310	0.257628
-45.021414	-2.147720	2.321818	0.008382	0.257935
-44.766195	-2.185439	2.331814	0.008334	0.257984
-44.635569	-2.191619	2.341811	0.008310	0.258082
-44.157623	-2.247754	2.351808	0.008221	0.258254
-44.347858	-2.212970	2.361805	0.008256	0.258255
-43.858556	-2.245911	2.371802	0.008165	0.258569
-43.538883	-2.304759	2.381798	0.008106	0.258565
-43.660738	-2.253261	2.391795	0.008129	0.258728
-43.472057	-2.260635	2.401792	0.008094	0.258879
-43.630516	-2.205975	2.411789	0.008123	0.259023
-43.107852	-2.265453	2.421786	0.008026	0.259221
-43.066581	-2.252416	2.431782	0.008018	0.259336
-42.947287	-2.243714	2.441779	0.007996	0.259505
-43.125330	-2.179369	2.451776	0.008029	0.259683
-42.793304	-2.211161	2.461773	0.007968	0.259842
-42.525643	-2.217509	2.471770	0.007918	0.260078
-42.472144	-2.211139	2.481766	0.007908	0.260167
-42.409592	-2.160525	2.491763	0.007897	0.260511
-41.950771	-2.230979	2.501760	0.007811	0.260583
-42.087465	-2.176215	2.511757	0.007837	0.260749
-41.601444	-2.225243	2.521754	0.007746	0.260967
-41.516127	-2.218298	2.531750	0.007731	0.261091
-41.324550	-2.204521	2.541747	0.007695	0.261360
-41.492017	-2.135602	2.551744	0.007726	0.261573
-40.822224	-2.233048	2.561741	0.007602	0.261708
-41.038460	-2.140607	2.571738	0.007642	0.262001
-40.747561	-2.158960	2.581734	0.007588	0.262191
-40.717904	-2.130688	2.591731	0.007582	0.262377
-40.334934	-2.153783	2.601728	0.007511	0.262633
-40.386223	-2.095374	2.611725	0.007521	0.262904
-40.170933	-2.096370	2.621722	0.007481	0.263113
-40.052319	-2.080737	2.631718	0.007459	0.263318
-39.557373	-2.120501	2.641715	0.007367	0.263593
-39.366657	-2.111477	2.651712	0.007331	0.263833
-39.729728	-2.003525	2.661709	0.007399	0.264063
-39.343007	-2.024885	2.671706	0.007327	0.264331
-38.736603	-2.097770	2.681702	0.007214	0.264535
-38.459766	-2.095076	2.691699	0.007163	0.264825
-38.933916	-1.960823	2.701696	0.007251	0.265087
-38.831255	-1.929020	2.711693	0.007232	0.265362
-37.845617	-2.067664	2.721690	0.007048	0.265583
-37.783116	-2.041748	2.731686	0.007037	0.265786
-37.340622	-2.068007	2.741683	0.006955	0.266081
-37.526594	-1.990067	2.751680	0.006989	0.266321
-37.282228	-1.988490	2.761677	0.006944	0.266570
-36.718526	-2.047730	2.771674	0.006839	0.266805
-36.246459	-2.093498	2.781670	0.006751	0.267022
-36.096269	-2.066427	2.791667	0.006723	0.267317
-35.869913	-2.066085	2.801664	0.006681	0.267541
-35.243661	-2.143946	2.811661	0.006565	0.267736
-34.718290	-2.191713	2.821658	0.006467	0.267994
-34.923906	-2.107675	2.831654	0.006505	0.268245
-34.564860	-2.136179	2.841651	0.006439	0.268443
-34.391024	-2.131161	2.851648	0.006406	0.268640
-34.017984	-2.148238	2.861645	0.006337	0.268913
-33.493752	-2.198548	2.871642	0.006239	0.269155
-33.567846	-2.148926	2.881638	0.006253	0.269349
-33.274570	-2.168096	2.891635	0.006199	0.269533
-32.910549	-2.175184	2.901632	0.006131	0.269850
-32.293173	-2.257707	2.911629	0.006016	0.270009
-32.201408	-2.240258	2.921626	0.005999	0.270191
-32.402979	-2.142456	2.931622	0.006037	0.270518
-31.823154	-2.213876	2.941619	0.005929	0.270700
-32.190349	-2.109986	2.951616	0.005997	0.270898
-31.187446	-2.259098	2.961613	0.005811	0.271076
-30.867664	-2.262792	2.971610	0.005751	0.271366
-31.129316	-2.179212	2.981606	0.005800	0.271558
-30.838611	-2.190798	2.991603	0.005746	0.271777
-30.667830	-2.176796	3.001600	0.005714	0.272017
-30.387197	-2.175439	3.011597	0.005662	0.272295
-30.390152	-2.134604	3.021594	0.005663	0.272509
-30.057512	-2.152658	3.031590	0.005601	0.272734
-29.873602	-2.134798	3.041587	0.005567	0.273006
-29.386362	-2.174356	3.051584	0.005476	0.273265
-29.008095	-2.202847	3.061581	0.005406	0.273478
-28.771284	-2.210474	3.071578	0.005362	0.273665
-28.489972	-2.214010	3.081574	0.005309	0.273917
-28.037128	-2.246198	3.091571	0.005225	0.274181
-28.068589	-2.205671	3.101568	0.005231	0.274365
-26.986886	-2.373382	3.111565	0.005030	0.274517
-27.309722	-2.256537	3.121562	0.005090	0.274823
-27.087885	-2.261691	3.131558	0.005049	0.275008
-27.048584	-2.229021	3.141555	0.005041	0.275217
-27.048688	-2.170640	3.151552	0.005042	0.275524
-26.464119	-2.240667	3.161549	0.004933	0.275714
-26.985092	-2.105076	3.171546	0.005030	0.275928
-26.411336	-2.164242	3.181542	0.004923	0.276165
-26.352695	-2.129729	3.191539	0.004912	0.276401
-26.219136	-2.091434	3.201536	0.004887	0.276728
-25.656021	-2.151499	3.211533	0.004783	0.276949
-25.768500	-2.086248	3.221530	0.004804	0.277183
-24.977447	-2.184535	3.231526	0.004656	0.277420
-25.044708	-2.125111	3.241523	0.004669	0.277666
-24.975010	-2.073838	3.251520	0.004656	0.277999
-24.367470	-2.141550	3.261517	0.004543	0.278221
-24.543609	-2.066636	3.271514	0.004576	0.278444
-24.085287	-2.099287	3.281510	0.004491	0.278707
-24.377013	-1.993565	3.291507	0.004545	0.278980
-23.592092	-2.080322	3.301504	0.004399	0.279270
-23.465920	-2.054367	3.311501	0.004376	0.279523
-22.788655	-2.133665	3.321498	0.004250	0.279749
-22.543511	-2.133392	3.331494	0.004204	0.279981
-22.383033	-2.119021	3.341491	0.004174	0.280205
-21.882978	-2.147607	3.351488	0.004081	0.280527
-21.809045	-2.129607	3.361485	0.004068	0.280689
-21.847792	-2.079644	3.371482	0.004075	0.280910
-21.682157	-2.058628	3.381478	0.004044	0.281173
-21.847633	-1.977751	3.391475	0.004075	0.281433
-20.890843	-2.093851	3.401472	0.003897	0.281731
-20.460889	-2.128968	3.411469	0.003817	0.281951
-20.033952	-2.169629	3.421466	0.003737	0.282141
-20.280859	-2.073816	3.431462	0.003783	0.282401
-19.860754	-2.099996	3.441459	0.003705	0.282658
-19.325116	-2.141265	3.451456	0.003606	0.282945
-19.519749	-2.062207	3.461453	0.003642	0.283168
-18.827991	-2.150947	3.471450	0.003513	0.283357
-18.517145	-2.159178	3.481446	0.003456	0.283603
-18.285476	-2.147971	3.491443	0.003412	0.283875
-18.145461	-2.129461	3.501440	0.003386	0.284098
-18.144444	-2.085824	3.511437	0.003386	0.284321
-17.908759	-2.084895	3.521434	0.003343	0.284543
-17.161490	-2.161568	3.531430	0.003203	0.284844
-16.982267	-2.157125	3.541427	0.003170	0.285032
-17.097315	-2.090543	3.551424	0.003192	0.285263
-17.099918	-2.035878	3.561421	0.003192	0.285538
-16.519524	-2.091628	3.571418	0.003084	0.285789
-16.422397	-2.065881	3.581414	0.003066	0.286009
-16.402247	-2.021501	3.591411	0.003063	0.286251
-15.746523	-2.099903	3.601408	0.002941	0.286457
-16.101902	-1.974527	3.611405	0.003007	0.286764
-15.385667	-2.051987	3.621402	0.002873	0.287029
-15.039405	-2.068594	3.631398	0.002809	0.287263
-14.805070	-2.067881	3.641395	0.002766	0.287480
-14.110239	-2.156528	3.651392	0.002636	0.287670
-14.442296	-2.026461	3.661389	0.002698	0.288020
-13.807326	-2.099504	3.671386	0.002580	0.288232
-13.943397	-2.031364	3.681382	0.002605	0.288450
-13.133805	-2.141802	3.691379	0.002455	0.288634
-12.684214	-2.167363	3.701376	0.002371	0.288915
-12.455658	-2.167876	3.711373	0.002329	0.289120
-12.488198	-2.116906	3.721370	0.002335	0.289345
-12.198068	-2.127311	3.731366	0.002281	0.289556
-11.954235	-2.115759	3.741363	0.002236	0.289835
-11.513828	-2.157348	3.751360	0.002154	0.290027
-10.835071	-2.250541	3.761357	0.002027	0.290177
-10.725852	-2.203871	3.771354	0.002007	0.290508
-10.799446	-2.161202	3.781350	0.002021	0.290653
-10.356126	-2.213335	3.791347	0.001938	0.290795
-10.187777	-2.181846	3.801344	0.001907	0.291103
-9.940858	-2.192810	3.811341	0.001861	0.291271
-9.804065	-2.179411	3.821338	0.001836	0.291461
-9.869166	-2.107501	3.831334	0.001848	0.291759
-8.986140	-2.226567	3.841331	0.001684	0.291964
-9.130759	-2.164171	3.851328	0.001711	0.292142
-8.728829	-2.194344	3.861325	0.001636	0.292354
-8.745105	-2.130366	3.871322	0.001639	0.292656
-8.312861	-2.169511	3.881318	0.001559	0.292850
-7.936157	-2.200315	3.891315	0.001489	0.293036
-7.717849	-2.189137	3.901312	0.001448	0.293287
-7.930581	-2.103859	3.911309	0.001488	0.293516
-7.825099	-2.075271	3.921306	0.001468	0.293751
-6.770458	-2.233631	3.931302	0.001272	0.293915
-6.994690	-2.123878	3.941299	0.001314	0.294254
-6.730762	-2.134325	3.951296	0.001265	0.294438
-7.006798	-2.040716	3.961293	0.001316	0.294651
-6.553306	-2.074396	3.971290	0.001232	0.294890
-6.409946	-2.034154	3.981286	0.001205	0.295215
-6.493676	-1.963042	3.991283	0.001221	0.295489
-5.705231	-2.069383	4.001280	0.001074	0.295669
-5.353090	-2.097262	4.011277	0.001008	0.295845
-5.212828	-2.070507	4.021274	0.000982	0.296101
-5.060548	-2.041837	4.031270	0.000954	0.296375
-4.969156	-2.008537	4.041267	0.000937	0.296619
-4.413276	-2.065296	4.051264	0.000834	0.296834
-4.199331	-2.064207	4.061261	0.000794	0.297029
-4.032510	-2.027725	4.071258	0.000763	0.297353
-3.857599	-2.013994	4.081254	0.000731	0.297574
-3.478627	-2.036947	4.091251	0.000660	0.297797
-3.735307	-1.936692	4.101248	0.000708	0.298057
-3.632460	-1.906880	4.111245	0.000689	0.298292
-2.809550	-1.991226	4.121242	0.000536	0.298608
-2.902659	-1.925528	4.131238	0.000553	0.298844
-2.875607	-1.875419	4.141235	0.000548	0.299110
-2.795462	-1.841964	4.151232	0.000533	0.299342
-2.501991	-1.841153	4.161229	0.000479	0.299603
-2.601132	-1.760762	4.171226	0.000497	0.299904
-2.313746	-1.753440	4.181222	0.000444	0.300190
-2.316414	-1.679888	4.191219	0.000444	0.300542
-2.493104	-1.597489	4.201216	0.000477	0.300784
-1.957384	-1.635190	4.211213	0.000377	0.301070
-2.413396	-1.489221	4.221210	0.000462	0.301373
-2.165285	-1.463494	4.231206	0.000416	0.301712
-1.733066	-1.478660	4.241203	0.000336	0.302016
-1.141724	-1.519338	4.251200	0.000226	0.302335
-1.407182	-1.399552	4.261197	0.000275	0.302677
-1.417098	-1.321794	4.271194	0.000277	0.303039
-1.664663	-1.205545	4.281190	0.000323	0.303379
-1.531065	-1.154224	4.291187	0.000298	0.303739
-1.257105	-1.130462	4.301184	0.000247	0.304089
-1.043605	-1.095752	4.311181	0.000208	0.304438
-0.687154	-1.085672	4.321178	0.000141	0.304793
-0.235790	-1.088474	4.331174	0.000058	0.305169
0.084181	-1.067528	4.341171	-0.000002	0.305543
-0.009062	-0.985049	4.351168	0.000015	0.305853
0.117695	-0.931306	4.361165	-0.000008	0.306215
0.210923	-0.868950	4.371162	-0.000025	0.306589
0.152447	-0.781626	4.381158	-0.000015	0.306951
0.133703	-0.685174	4.391155	-0.000011	0.307389
0.256690	-0.621487	4.401152	-0.000034	0.307793
0.037639	-0.499685	4.411149	0.000007	0.308178
0.461686	-0.482830	4.421146	-0.000072	0.308618
0.318118	-0.360281	4.431142	-0.000045	0.309069
0.929644	-0.391127	4.441139	-0.000159	0.309445
0.761049	-0.259524	4.451136	-0.000128	0.309916
0.847635	-0.182572	4.461133	-0.000144	0.310348
0.223832	0.027762	4.471130	-0.000028	0.310799
0.000000	0.168902	4.481126	0.000014	0.311266

-0.238565	0.486424	4.486131	0.000058	0.312538
0.635877	0.881673	4.491136	-0.000105	0.315093
1.178334	1.632066	4.496141	-0.000206	0.318966
2.051529	2.613599	4.501146	-0.000369	0.324096
3.554996	3.784670	4.506150	-0.000650	0.330479
4.364781	5.382765	4.511155	-0.000802	0.338032
5.759070	7.177682	4.516160	-0.001063	0.346686
8.504067	9.050892	4.521165	-0.001575	0.356442
10.090657	11.454292	4.526170	-0.001872	0.367201
11.710717	14.192037	4.531174	-0.002175	0.378954
14.493608	17.061392	4.536179	-0.002695	0.391619
17.481062	20.245159	4.541184	-0.003254	0.405141
20.772962	23.746717	4.546189	-0.003869	0.419512
25.197203	27.417238	4.551194	-0.004695	0.434651
29.683751	31.466000	4.556198	-0.005533	0.450527
34.321890	35.879057	4.561203	-0.006399	0.467074
39.813418	40.528508	4.566208	-0.007425	0.484218
44.978562	45.649444	4.571213	-0.008390	0.501960
49.104478	51.344307	4.576218	-0.009162	0.520167
54.200358	57.229198	4.581222	-0.010115	0.538734
60.454319	63.286917	4.586227	-0.011283	0.557665
67.759189	69.534084	4.591232	-0.012647	0.576917
75.611755	76.078101	4.596237	-0.014114	0.596498
87.988072	82.174592	4.601242	-0.016422	0.616302
139.692480	81.821030	4.606246	-0.026049	0.636825
160.819371	87.864194	4.611251	-0.029987	0.658688
162.741915	97.608608	4.616256	-0.030351	0.680402
164.093607	107.631372	4.621261	-0.030609	0.701804
165.633927	117.747370	4.626266	-0.030903	0.722825
167.569205	127.925688	4.631270	-0.031270	0.743506
169.759894	138.129300	4.636275	-0.031684	0.763759
171.857471	148.430849	4.641280	-0.032081	0.783636
174.054938	158.774934	4.646285	-0.032497	0.803128
175.957200	169.194554	4.651290	-0.032858	0.822196
178.419230	179.531422	4.656294	-0.033323	0.840858
179.873323	190.024189	4.661299	-0.033601	0.859076
181.515580	200.454863	4.666304	-0.033913	0.876866
183.334504	210.814960	4.671309	-0.034259	0.894238
184.970960	221.159112	4.676314	-0.034570	0.911201
187.280725	231.327617	4.681318	-0.035007	0.927764
188.867621	241.564665	4.686323	-0.035309	0.943945
189.948675	251.810818	4.691328	-0.035517	0.959734
191.481205	261.899586	4.696333	-0.035809	0.975150
193.078925	271.903401	4.701338	-0.036113	0.990218
194.655043	281.818038	4.706342	-0.036413	1.004926
195.224983	291.816575	4.711347	-0.036525	1.019292
197.110939	301.475460	4.716352	-0.036883	1.033303
198.436059	311.174384	4.721357	-0.037136	1.047046
200.127451	320.718328	4.726362	-0.037457	1.060487
201.195078	330.316953	4.731366	-0.037662	1.073686
202.152462	339.825729	4.736371	-0.037846	1.086581
203.469795	349.204666	4.741376	-0.038098	1.099235
204.900086	358.499762	4.746381	-0.038370	1.111660
206.345833	367.698359	4.751386	-0.038645	1.123828
207.664852	376.894675	4.756390	-0.038897	1.135833
208.973146	386.022935	4.761395	-0.039146	1.147625
209.952143	395.154098	4.766400	-0.039334	1.159229
210.864196	404.231123	4.771405	-0.039510	1.170638
211.690240	413.240822	4.776410	-0.039670	1.181835
212.670712	422.189865	4.781414	-0.039858	1.192886
213.172009	431.156197	4.786419	-0.039957	1.203758
213.997431	440.014129	4.791424	-0.040117	1.214469
215.156307	448.778295	4.796429	-0.040338	1.225043
215.694278	457.607152	4.801434	-0.040444	1.235478
216.380367	466.355737	4.806438	-0.040577	1.245762
216.956017	475.096877	4.811443	-0.040690	1.255931
217.701650	483.757049	4.816448	-0.040835	1.265958
218.193590	492.462581	4.821453	-0.040932	1.275910
219.343391	500.975165	4.826458	-0.041151	1.285692
220.477400	509.523328	4.831462	-0.041368	1.295437
221.368710	518.070841	4.836467	-0.041540	1.305062
221.935703	526.740681	4.841472	-0.041651	1.314691
222.999429	535.197063	4.846477	-0.041854	1.324108
223.617775	543.719287	4.851482	-0.041975	1.333449
223.777875	552.293753	4.856486	-0.042010	1.342698
224.399478	560.761138	4.861491	-0.042132	1.351852
225.129746	569.170702	4.866496	-0.042273	1.360903
225.849179	577.606613	4.871501	-0.042412	1.369919
226.835723	585.966280	4.876506	-0.042602	1.378842
227.222481	594.453474	4.881510	-0.042679	1.387736
227.709841	602.865772	4.886515	-0.042775	1.396514
228.000359	611.289483	4.891520	-0.042835	1.405215
229.362940	619.537189	4.896525	-0.043094	1.413864
229.974244	627.908256	4.901530	-0.043213	1.422459
230.393689	636.319327	4.906534	-0.043297	1.431010
231.363143	644.602814	4.911539	-0.043482	1.439473
232.453466	652.851679	4.916544	-0.043691	1.447872
233.000307	661.234813	4.921549	-0.043798	1.456266
233.702508	669.556739	4.926554	-0.043934	1.464577
235.023251	677.811612	4.931558	-0.044185	1.472875
235.851258	686.110725	4.936563	-0.044345	1.481090
236.048414	694.505542	4.941568	-0.044387	1.489252
236.672681	702.833464	4.946573	-0.044509	1.497372
237.530386	711.053332	4.951578	-0.044674	1.505381
238.674098	719.280658	4.956582	-0.044892	1.513399
239.417915	727.546380	4.961587	-0.045036	1.521349
240.008134	735.841541	4.966592	-0.045151	1.529262
240.673814	744.141183	4.971597	-0.045280	1.537149
241.539706	752.357256	4.976602	-0.045447	1.544948
242.358186	760.638847	4.981606	-0.045605	1.552762
242.517020	768.979514	4.986611	-0.045640	1.560491
242.848506	777.259133	4.991616	-0.045707	1.568153
243.779681	785.461214	4.996621	-0.045886	1.575794
244.310409	793.717381	5.001626	-0.045990	1.583389
245.961809	801.805019	5.006630	-0.046302	1.590958
246.768606	810.041267	5.011635	-0.046458	1.598502
247.468304	818.270153	5.016640	-0.046594	1.605989
247.902210	826.583984	5.021645	-0.046680	1.613478
248.833584	834.744224	5.026650	-0.046858	1.620867
249.751974	842.968584	5.031654	-0.047035	1.628276
250.362838	851.226037	5.036659	-0.047154	1.635638
250.979712	859.435397	5.041664	-0.047274	1.642925
251.359742	867.700589	5.046669	-0.047350	1.650196
251.882448	875.935696	5.051674	-0.047453	1.657428
252.950394	884.050819	5.056678	-0.047657	1.664600
253.645358	892.254940	5.061683	-0.047792	1.671766
254.395585	900.455670	5.066688	-0.047937	1.678906
255.509554	908.565823	5.071693	-0.048149	1.685988
255.820080	916.845591	5.076698	-0.048212	1.693075
256.201582	925.086626	5.081702	-0.048289	1.700110
256.794881	933.287811	5.086707	-0.048405	1.707110
257.851041	941.386995	5.091712	-0.048606	1.714056
258.783788	949.529172	5.096717	-0.048785	1.720995
259.150324	957.764713	5.101722	-0.048859	1.727908
259.809219	965.952090	5.106726	-0.048987	1.734792
260.442836	974.115969	5.111731	-0.049110	1.741626
261.355572	982.256867	5.116736	-0.049285	1.748450
262.212833	990.416544	5.121741	-0.049450	1.755256
262.311537	998.661438	5.126746	-0.049474	1.762007
263.126998	1006.802493	5.131750	-0.049631	1.768740
263.489620	1015.033541	5.136755	-0.049704	1.775462
264.247415	1023.145576	5.141760	-0.049850	1.782113
264.581616	1031.397745	5.146765	-0.049918	1.788798
265.142164	1039.554717	5.151770	-0.050028	1.795410
265.962150	1047.660579	5.156774	-0.050186	1.801989
266.472447	1055.825654	5.161779	-0.050286	1.808552
267.165853	1063.958267	5.166784	-0.050420	1.815089
267.892049	1072.094062	5.171789	-0.050561	1.821608
268.355434	1080.249089	5.176794	-0.050652	1.828087
268.399857	1088.515870	5.181798	-0.050666	1.834580
269.651819	1096.489043	5.186803	-0.050904	1.840967
270.218652	1104.639436	5.191808	-0.051015	1.847386
270.901166	1112.785061	5.196813	-0.051147	1.853793
271.427564	1120.945905	5.201818	-0.051251	1.860171
272.315860	1129.063402	5.206822	-0.051421	1.866537
273.322689	1137.147580	5.211827	-0.051614	1.872869
273.382061	1145.395076	5.216832	-0.051630	1.879193
274.175399	1153.479353	5.221837	-0.051783	1.885457
274.775440	1161.617851	5.226842	-0.051900	1.891719
274.733133	1169.881058	5.231846	-0.051898	1.897981
275.440418	1177.955596	5.236851	-0.052035	1.904165
276.238767	1186.060651	5.241856	-0.052189	1.910363
276.990765	1194.167105	5.246861	-0.052334	1.916536
277.914948	1202.226274	5.251866	-0.052511	1.922673
278.807211	1210.332998	5.256870	-0.052683	1.928822
279.063508	1218.530300	5.261875	-0.052736	1.934948
279.543233	1226.664874	5.266880	-0.052830	1.941032
280.569247	1234.754547	5.271885	-0.053026	1.947125
280.617607	1242.981695	5.276890	-0.053041	1.953192
281.279367	1251.046539	5.281894	-0.053169	1.959188
282.186800	1259.093414	5.286899	-0.053343	1.965179
283.202309	1267.130390	5.291904	-0.053538	1.971157
283.897830	1275.287588	5.296909	-0.053672	1.977169
283.898403	1283.492638	5.301914	-0.053678	1.983122
285.118325	1291.525682	5.306918	-0.053910	1.989064
285.858354	1299.638856	5.311923	-0.054053	1.994995
286.336066	1307.772378	5.316928	-0.054147	2.000894
287.111769	1315.880359	5.321933	-0.054297	2.006789
287.787113	1324.001288	5.326938	-0.054428	2.012665
288.853655	1332.053442	5.331942	-0.054632	2.018516
289.714181	1340.141009	5.336947	-0.054797	2.024354
289.846775	1348.366679	5.341952	-0.054827	2.030196
290.754445	1356.420304	5.346957	-0.055002	2.035981
291.064295	1364.571548	5.351962	-0.055065	2.041755
291.954820	1372.636156	5.356966	-0.055236	2.047513
292.537478	1380.771044	5.361971	-0.055349	2.053271
293.279454	1388.844326	5.366976	-0.055493	2.058987
294.494186	1396.855615	5.371981	-0.055724	2.064691
295.283993	1404.953418	5.376986	-0.055876	2.070397
295.847535	1413.123328	5.381990	-0.055987	2.076113
296.337100	1421.246026	5.386995	-0.056083	2.081774
296.398138	1429.451479	5.392000	-0.056100	2.087433
297.203916	1437.514590	5.397005	-0.056255	2.093054
297.998552	1445.587507	5.402010	-0.056408	2.098665
298.635685	1453.689998	5.407014	-0.056532	2.104265
299.237298	1461.821122	5.412019	-0.056649	2.109866
299.950659	1469.926192	5.417024	-0.056787	2.115446
301.064236	1477.938385	5.422029	-0.057000	2.120986
302.071455	1485.963505	5.427034	-0.057193	2.126511
302.828116	1494.055478	5.432038	-0.057339	2.132042
303.399934	1502.181057	5.437043	-0.057450	2.137562
303.842673	1510.291688	5.442048	-0.057538	2.143046
304.246081	1518.456664	5.447053	-0.057619	2.148549
304.921332	1526.551906	5.452058	-0.057750	2.154016
305.676642	1534.595501	5.457062	-0.057895	2.159443
306.312736	1542.680272	5.462067	-0.058019	2.164873
306.758630	1550.810180	5.467072	-0.058107	2.170300
307.648337	1558.883984	5.472077	-0.058278	2.175718
308.934817	1566.867997	5.477082	-0.058523	2.181101
309.592734	1574.990441	5.482086	-0.058651	2.186502
310.310082	1583.109067	5.487091	-0.058789	2.191893
310.661752	1591.228204	5.492096	-0.058860	2.197237
311.459608	1599.279256	5.497101	-0.059014	2.202565
311.807396	1607.399683	5.502106	-0.059084	2.207883
313.196100	1615.376763	5.507110	-0.059348	2.213191
313.383676	1623.582345	5.512115	-0.059388	2.218524
314.133716	1631.604519	5.517120	-0.059533	2.223777
314.550336	1639.775066	5.522125	-0.059616	2.229083
315.474050	1647.780927	5.527130	-0.059793	2.234316
315.712167	1655.909980	5.532134	-0.059842	2.239554
316.384042	1663.974288	5.537139	-0.059973	2.244777
316.596945	1672.121847	5.542144	-0.060018	2.249999
317.536223	1680.164461	5.547149	-0.060198	2.255208
317.824137	1688.280354	5.552154	-0.060257	2.260393
318.190978	1696.369119	5.557158	-0.060330	2.265556
319.253257	1704.396659	5.562163	-0.060533	2.270729
319.490762	1712.528892	5.567168	-0.060583	2.275884
320.037822	1720.594631	5.572173	-0.060690	2.281013
320.280975	1728.684968	5.577178	-0.060740	2.286119
321.006930	1736.724550	5.582182	-0.060881	2.291224
321.782567	1744.776723	5.587187	-0.061030	2.296329
322.457584	1752.818949	5.592192	-0.061161	2.301408
323.266523	1760.869761	5.597197	-0.061317	2.306492
323.092420	1769.085682	5.602202	-0.061290	2.311584
323.709898	1777.130011	5.607206	-0.061410	2.316625
325.320426	1785.031626	5.612211	-0.061715	2.321651
325.865475	1793.148015	5.617216	-0.061822	2.326709
326.371496	1801.254818	5.622221	-0.061921	2.331746
327.021642	1809.314589	5.627226	-0.062047	2.336755
327.530706	1817.412879	5.632230	-0.062148	2.341766
328.333929	1825.450024	5.637235	-0.062302	2.346752
328.546566	1833.606093	5.642240	-0.062347	2.351752
329.256096	1841.653000	5.647245	-0.062484	2.356715
329.920457	1849.685978	5.652250	-0.062613	2.361656
330.410383	1857.772981	5.657254	-0.062710	2.366604
331.039387	1865.862587	5.662259	-0.062832	2.371555
331.261985	1873.972157	5.667264	-0.062879	2.376475
332.054974	1881.991774	5.672269	-0.063032	2.381376
332.368348	1890.094295	5.677274	-0.063095	2.386278
332.823576	1898.206866	5.682278	-0.063185	2.391188
333.175978	1906.289222	5.687283	-0.063256	2.396061
333.797404	1914.290851	5.692288	-0.063377	2.400897
334.264839	1922.381464	5.697293	-0.063469	2.405764
334.913084	1930.430535	5.702298	-0.063595	2.410611
336.044087	1938.404264	5.707302	-0.063811	2.415442
336.608176	1946.514986	5.712307	-0.063921	2.420299
336.753412	1954.631587	5.717312	-0.063954	2.425117
337.801238	1962.649347	5.722317	-0.064154	2.429937
339.109692	1970.627717	5.727322	-0.064403	2.434745
339.561898	1978.735819	5.732326	-0.064492	2.439553
339.780075	1986.850994	5.737331	-0.064538	2.444337
340.427856	1994.890340	5.742336	-0.064664	2.449100
341.107052	2002.966198	5.747341	-0.064795	2.453878
341.330178	2011.066895	5.752346	-0.064842	2.458626
342.022928	2019.095160	5.757350	-0.064976	2.463359
343.135748	2027.069169	5.762355	-0.065189	2.468082
343.688050	2035.164368	5.767360	-0.065297	2.472825
344.251591	2043.237335	5.772365	-0.065407	2.477546
344.373060	2051.355175	5.777370	-0.065435	2.482250
344.851994	2059.431603	5.782374	-0.065529	2.486948
344.981197	2067.585430	5.787379	-0.065559	2.491656
345.707294	2075.577187	5.792384	-0.065699	2.496307
346.144356	2083.640622	5.797389	-0.065786	2.500968
346.303030	2091.742928	5.802394	-0.065820	2.505622
346.330466	2099.870290	5.807398	-0.065831	2.510272
346.919677	2107.891979	5.812403	-0.065946	2.514894
347.794795	2115.807457	5.817408	-0.066114	2.519468
348.097871	2123.895642	5.822413	-0.066175	2.524091
348.870389	2131.918100	5.827418	-0.066324	2.528701
349.658415	2139.963354	5.832422	-0.066476	2.533317
350.316145	2148.034145	5.837427	-0.066604	2.537930
350.892358	2156.064335	5.842432	-0.066716	2.542505
351.669349	2164.118624	5.847437	-0.066866	2.547100
351.684602	2172.269077	5.852442	-0.066874	2.551685
352.046132	2180.348062	5.857446	-0.066947	2.556248
352.870547	2188.348524	5.862451	-0.067106	2.560790
353.189204	2196.393624	5.867456	-0.067170	2.565314
353.866360	2204.475912	5.872461	-0.067302	2.569876
354.582241	2212.474764	5.877466	-0.067440	2.574386
354.623124	2220.630164	5.882470	-0.067453	2.578927
355.174934	2228.686246	5.887475	-0.067561	2.583442
355.678189	2236.707668	5.892480	-0.067660	2.587925
356.164876	2244.889340	5.897485	-0.067756	2.592488
356.212604	2252.997843	5.902490	-0.067770	2.596972
356.769900	2260.953655	5.907494	-0.067879	2.601400
357.385987	2268.953732	5.912499	-0.067999	2.605848
357.878927	2276.973035	5.917504	-0.068096	2.610291
358.634868	2285.008762	5.922509	-0.068242	2.614753
358.813335	2293.077078	5.927514	-0.068280	2.619185
359.301974	2301.112566	5.932518	-0.068376	2.623613
360.098835	2309.111319	5.937523	-0.068530	2.628035
360.405879	2317.203449	5.942528	-0.068592	2.632467
360.796049	2325.273270	5.947533	-0.068670	2.636884
360.877746	2333.362243	5.952538	-0.068690	2.641284
361.816768	2341.328340	5.957542	-0.068870	2.645667
362.497905	2349.388495	5.962547	-0.069002	2.650077
362.961523	2357.447073	5.967552	-0.069094	2.654464
363.276277	2365.544514	5.972557	-0.069158	2.658854
363.474541	2373.615313	5.977562	-0.069200	2.663215
364.139977	2381.632934	5.982566	-0.069329	2.667571
365.057213	2389.648392	5.987571	-0.069505	2.671936
365.478072	2397.715400	5.992576	-0.069589	2.676288
366.073706	2405.758139	5.997581	-0.069705	2.680631
366.347190	2413.827771	6.002586	-0.069761	2.684961
366.896706	2421.858307	6.007590	-0.069868	2.689280
367.478906	2429.906922	6.012595	-0.069982	2.693605
368.224711	2437.896705	6.017600	-0.070126	2.697901
368.809146	2445.958032	6.022605	-0.070240	2.702218
369.475687	2453.996751	6.027610	-0.070369	2.706522
369.452017	2462.167294	6.032614	-0.070370	2.710844
370.059889	2470.201533	6.037619	-0.070489	2.715127
370.569094	2478.199668	6.042624	-0.070589	2.719378
370.706499	2486.293191	6.047629	-0.070619	2.723649
371.220998	2494.328202	6.052634	-0.070720	2.727907
371.535261	2502.401204	6.057638	-0.070784	2.732165
372.013492	2510.438807	6.062643	-0.070878	2.736408
372.142398	2518.512891	6.067648	-0.070908	2.740642
372.946154	2526.502510	6.072653	-0.071063	2.744867
373.357084	2534.539593	6.077658	-0.071144	2.749086
373.650299	2542.697990	6.082662	-0.071204	2.753354
374.118167	2550.724803	6.087667	-0.071296	2.757558
374.316419	2558.739455	6.092672	-0.071339	2.761732
374.835337	2566.761656	6.097677	-0.071440	2.765924
375.273632	2574.802208	6.102682	-0.071527	2.770113
375.741825	2582.855906	6.107686	-0.071620	2.774305
376.433638	2590.867359	6.112691	-0.071754	2.778482
376.654958	2598.915498	6.117696	-0.071800	2.782644
377.322583	2606.951524	6.122701	-0.071929	2.786819
377.691262	2615.001470	6.127706	-0.072003	2.790978
377.672205	2623.133821	6.132710	-0.072005	2.795149
378.117205	2631.145011	6.137715	-0.072093	2.799280
378.574549	2639.147314	6.142720	-0.072183	2.803401
379.200600	2647.159821	6.147725	-0.072305	2.807530
380.122005	2655.136799	6.152730	-0.072482	2.811653
380.863252	2663.178747	6.157734	-0.072625	2.815793
381.290344	2671.283965	6.162739	-0.072710	2.819939
381.420334	2679.340225	6.167744	-0.072739	2.824037
382.310368	2687.365202	6.172749	-0.072910	2.828158
383.004286	2695.381715	6.177754	-0.073045	2.832257
383.402016	2703.447284	6.182758	-0.073124	2.836358
383.651207	2711.564036	6.187763	-0.073176	2.840469
384.080722	2719.530776	6.192768	-0.073261	2.844510
384.788574	2727.555552	6.197773	-0.073398	2.848590
384.997009	2735.677069	6.202778	-0.073442	2.852683
385.319210	2743.727727	6.207782	-0.073507	2.856742
385.338416	2751.826269	6.212787	-0.073516	2.860802
385.465220	2759.872333	6.217792	-0.073545	2.864836
386.206687	2767.859064	6.222797	-0.073688	2.868869
386.573966	2775.882158	6.227802	-0.073761	2.872894
387.330894	2783.867793	6.232806	-0.073907	2.876916
387.756905	2791.944939	6.237811	-0.073992	2.880959
387.878633	2800.003715	6.242816	-0.074020	2.884971
388.718083	2807.990186	6.247821	-0.074181	2.888981
388.483009	2816.170866	6.252826	-0.074143	2.893022
389.332319	2824.102218	6.257830	-0.074306	2.896993
389.742954	2832.178552	6.262835	-0.074388	2.901007
390.096504	2840.187190	6.267840	-0.074459	2.904979
390.129971	2848.328135	6.272845	-0.074470	2.908992
390.504642	2856.380293	6.277850	-0.074545	2.912975
390.449444	2864.449319	6.282854	-0.074540	2.916938
391.306001	2872.383333	6.287859	-0.074705	2.920878
391.688991	2880.378863	6.292864	-0.074781	2.924817
391.992798	2888.452831	6.297869	-0.074843	2.928785
392.362433	2896.514066	6.302874	-0.074917	2.932745
392.532020	2904.582113	6.307878	-0.074954	2.936692
392.706913	2912.631052	6.312883	-0.074992	2.940625
393.029780	2920.633615	6.317888	-0.075057	2.944538
393.611561	2928.674653	6.322893	-0.075171	2.948478
393.515210	2936.772334	6.327898	-0.075158	2.952404
394.276867	2944.716562	6.332902	-0.075305	2.956296
394.821718	2952.747471	6.337907	-0.075411	2.960213
395.108681	2960.746194	6.342912	-0.075470	2.964096
395.491038	2968.817702	6.347917	-0.075546	2.968014
395.767666	2976.864863	6.352922	-0.075603	2.971909
396.258623	2984.911963	6.357926	-0.075700	2.975811
396.712120	2992.927808	6.362931	-0.075789	2.979690
396.697623	3001.000047	6.367936	-0.075792	2.983566
397.171633	3009.046055	6.372941	-0.075885	2.987451
397.752729	3017.050912	6.377946	-0.075999	2.991316
397.936654	3025.131702	6.382950	-0.076038	2.995192
398.348023	3033.155674	6.387955	-0.076120	2.999047
399.000654	3041.126561	6.392960	-0.076247	3.002885
399.242733	3049.224348	6.397965	-0.076297	3.006756
399.382861	3057.295608	6.402970	-0.076328	3.010606
399.671891	3065.280040	6.407974	-0.076387	3.014416
400.402521	3073.286655	6.412979	-0.076529	3.018254
400.892758	3081.314701	6.417984	-0.076625	3.022085
401.288257	3089.404067	6.422989	-0.076704	3.025936
401.087116	3097.515754	6.427994	-0.076672	3.029763
401.362202	3105.516916	6.432998	-0.076728	3.033556
401.659832	3113.574222	6.438003	-0.076789	3.037372
402.262727	3121.548286	6.443008	-0.076906	3.041159
402.362176	3129.610314	6.448013	-0.076930	3.044958
402.752253	3137.632293	6.453018	-0.077008	3.048747
403.283096	3145.653172	6.458022	-0.077112	3.052538
403.698116	3153.711637	6.463027	-0.077194	3.056337
403.711163	3161.751216	6.468032	-0.077202	3.060102
404.472861	3169.728753	6.473037	-0.077349	3.063869
404.714271	3177.822968	6.478042	-0.077399	3.067662
405.128818	3185.889434	6.483046	-0.077481	3.071445
405.747403	3193.916960	6.488051	-0.077602	3.075214
406.371072	3201.861504	6.493056	-0.077723	3.078941
406.807937	3209.891565	6.498061	-0.077810	3.082694
407.293464	3217.910526	6.503066	-0.077905	3.086440
407.498389	3225.986939	6.508070	-0.077949	3.090194
407.951852	3234.027776	6.513075	-0.078038	3.093939
407.989465	3242.062038	6.518080	-0.078050	3.097656
408.189116	3250.163275	6.523085	-0.078093	3.101408
408.176993	3258.215947	6.528090	-0.078096	3.105123
408.668315	3266.211199	6.533094	-0.078192	3.108830
409.259136	3274.266637	6.538099	-0.078308	3.112565
409.469248	3282.253450	6.543104	-0.078352	3.116247
409.584148	3290.324682	6.548109	-0.078379	3.119958
409.626682	3298.352897	6.553114	-0.078392	3.123642
410.348309	3306.304351	6.558118	-0.078531	3.127318
410.943133	3314.384005	6.563123	-0.078647	3.131042
411.217418	3322.389286	6.568128	-0.078703	3.134713
411.590769	3330.451744	6.573133	-0.078778	3.138410
412.112779	3338.444077	6.578138	-0.078881	3.142077
412.286832	3346.531209	6.583142	-0.078918	3.145768
412.153094	3354.666566	6.588147	-0.078899	3.149462
412.788499	3362.596725	6.593152	-0.079022	3.153093
413.584335	3370.588726	6.598157	-0.079175	3.156755
413.651841	3378.697743	6.603162	-0.079193	3.160434
414.201156	3386.628290	6.608166	-0.079301	3.164048
414.821950	3394.668278	6.613171	-0.079421	3.167711
414.702033	3402.807448	6.618176	-0.079404	3.171382
415.031494	3410.819457	6.623181	-0.079471	3.175011
415.926219	3418.747058	6.628186	-0.079643	3.178623
415.900656	3426.829590	6.633190	-0.079643	3.182260
416.405715	3434.859588	6.638195	-0.079742	3.185892
416.540609	3442.914589	6.643200	-0.079773	3.189515
416.952655	3450.969520	6.648205	-0.079854	3.193146
417.128668	3458.997972	6.653210	-0.079892	3.196750
417.526338	3466.983592	6.658214	-0.079972	3.200341
417.881783	3475.027152	6.663219	-0.080043	3.203952
418.233861	3483.074698	6.668224	-0.080114	3.207561
418.892779	3491.120425	6.673229	-0.080242	3.211177
419.173098	3499.138683	6.678234	-0.080299	3.214761
419.650735	3507.143778	6.683238	-0.080393	3.218344
420.054183	3515.200209	6.688243	-0.080474	3.221942
419.950291	3523.266720	6.693248	-0.080459	3.225519
420.452481	3531.285618	6.698253	-0.080558	3.229096
420.452741	3539.385639	6.703258	-0.080563	3.232685
420.953213	3547.363632	6.708262	-0.080662	3.236236
421.032435	3555.411370	6.713267	-0.080682	3.239797
421.354606	3563.373098	6.718272	-0.080747	3.243326
421.903266	3571.386238	6.723277	-0.080854	3.246882
422.317642	3579.426638	6.728282	-0.080937	3.250442
422.503548	3587.465381	6.733286	-0.080976	3.253987
422.462650	3595.602975	6.738291	-0.080974	3.257563
423.170018	3603.541450	6.743296	-0.081111	3.261078
423.596675	3611.516223	6.748301	-0.081195	3.264593
423.856962	3619.591439	6.753306	-0.081249	3.268142
424.251418	3627.619680	6.758310	-0.081328	3.271671
424.733851	3635.669428	6.763315	-0.081423	3.275210
424.686947	3643.696548	6.768320	-0.081419	3.278714
424.953944	3651.740755	6.773325	-0.081474	3.282234
425.151197	3659.778598	6.778330	-0.081516	3.285745
425.546666	3667.771926	6.783334	-0.081595	3.289240
425.896899	3675.822604	6.788339	-0.081665	3.292755
426.063161	3683.875018	6.793344	-0.081702	3.296259
426.889342	3691.842532	6.798349	-0.081860	3.299749
426.839758	3699.931846	6.803354	-0.081856	3.303254
427.731291	3707.865577	6.808358	-0.082028	3.306724
428.381678	3715.946035	6.813363	-0.082154	3.310244
428.549394	3723.972448	6.818368	-0.082190	3.313719
429.580507	3731.914887	6.823373	-0.082388	3.317187
429.540066	3740.079224	6.828378	-0.082385	3.320705
430.101823	3747.995466	6.833382	-0.082495	3.324136
430.389935	3756.099865	6.838387	-0.082554	3.327634
430.744777	3764.128526	6.843392	-0.082625	3.331098
431.449082	3772.141333	6.848397	-0.082761	3.334565
431.484723	3780.222622	6.853402	-0.082773	3.338032
431.797696	3788.237589	6.858406	-0.082837	3.341478
432.163747	3796.259967	6.863411	-0.082910	3.344926
432.818450	3804.237715	6.868416	-0.083037	3.348361
432.848405	3812.371557	6.873421	-0.083048	3.351836
432.558536	3820.496409	6.878426	-0.082999	3.355292
433.025891	3828.415469	6.883430	-0.083091	3.358685
433.312147	3836.436276	6.888435	-0.083150	3.362110
433.410254	3844.455298	6.893440	-0.083173	3.365525
434.146357	3852.425077	6.898445	-0.083316	3.368938
433.900391	3860.551412	6.903450	-0.083275	3.372379
434.232972	3868.570517	6.908454	-0.083342	3.375792
434.896648	3876.529614	6.913459	-0.083471	3.379187
435.167384	3884.561015	6.918464	-0.083527	3.382596
435.987294	3892.546259	6.923469	-0.083684	3.386001
435.670406	3900.696189	6.928474	-0.083631	3.389432
436.036837	3908.721976	6.933478	-0.083704	3.392831
436.329059	3916.767489	6.938483	-0.083764	3.396233
436.476348	3924.754128	6.943488	-0.083796	3.399601
437.103330	3932.710401	6.948493	-0.083918	3.402969
436.945188	3940.819937	6.953498	-0.083894	3.406372
437.463242	3948.782341	6.958502	-0.083996	3.409732
437.774556	3956.867053	6.963507	-0.084059	3.413134
437.803103	3964.894221	6.968512	-0.084069	3.416498
438.337608	3972.872078	6.973517	-0.084174	3.419855
438.412350	3980.934498	6.978522	-0.084193	3.423229
439.079893	3988.911447	6.983526	-0.084323	3.426584
439.621436	3996.944428	6.988531	-0.084429	3.429955
439.848972	4004.960640	6.993536	-0.084476	3.433305
440.603389	4012.982497	6.998541	-0.084622	3.436672
440.933839	4021.011507	7.003546	-0.084688	3.440023
440.764694	4029.083595	7.008550	-0.084662	3.443373
441.439607	4037.080663	7.013555	-0.084793	3.446716
441.561598	4045.146900	7.018560	-0.084821	3.450066
442.070174	4053.137464	7.023565	-0.084921	3.453395
442.895616	4061.121483	7.028570	-0.085080	3.456729
442.841015	4069.207033	7.033574	-0.085075	3.460071
443.039781	4077.269257	7.038579	-0.085117	3.463409
443.284337	4085.272853	7.043584	-0.085168	3.466721
444.053730	4093.267627	7.048589	-0.085316	3.470044
444.718108	4101.295564	7.053594	-0.085445	3.473373
444.880020	4109.348345	7.058598	-0.085480	3.476693
444.758256	4117.446060	7.063603	-0.085463	3.480019
445.036030	4125.390296	7.068608	-0.085520	3.483292
445.482614	4133.397936	7.073613	-0.085608	3.486593
445.780293	4141.433600	7.078618	-0.085669	3.489898
445.971354	4149.511407	7.083622	-0.085710	3.493213
446.163358	4157.559513	7.088627	-0.085751	3.496513
445.924279	4165.627189	7.093632	-0.085711	3.499804
446.376897	4173.587488	7.098637	-0.085801	3.503070
446.562005	4181.644560	7.103642	-0.085840	3.506364
446.784816	4189.633570	7.108646	-0.085887	3.509629
447.532344	4197.647402	7.113651	-0.086031	3.512917
447.831402	4205.663374	7.118656	-0.086092	3.516188
449.007227	4213.555791	7.123661	-0.086316	3.519434
449.228206	4221.633911	7.128666	-0.086363	3.522722
449.012143	4229.757345	7.133670	-0.086328	3.526012
449.601518	4237.762179	7.138675	-0.086443	3.529276
449.591466	4245.799244	7.143680	-0.086446	3.532531
449.922600	4253.857669	7.148685	-0.086513	3.535802
450.023338	4261.888051	7.153690	-0.086537	3.539052
450.972267	4269.800768	7.158694	-0.086719	3.542277
451.607504	4277.830953	7.163699	-0.086842	3.545537
451.366611	4285.982661	7.168704	-0.086802	3.548816
452.147831	4293.966634	7.173709	-0.086953	3.552056
452.333254	4302.023481	7.178714	-0.086993	3.555304
452.966831	4309.959218	7.183718	-0.087116	3.558513
453.041671	4318.068850	7.188723	-0.087135	3.561773
453.077922	4326.080660	7.193728	-0.087147	3.564989
453.639719	4334.075217	7.198733	-0.087257	3.568211
454.155229	4342.105670	7.203738	-0.087358	3.571444
454.408127	4350.091382	7.208742	-0.087410	3.574647
454.532679	4358.174365	7.213747	-0.087439	3.577883
455.426989	4366.138165	7.218752	-0.087610	3.581091
455.947487	4374.090947	7.223757	-0.087712	3.584280
456.685416	4382.122776	7.228762	-0.087855	3.587505
456.928960	4390.251009	7.233766	-0.087906	3.590750
457.228246	4398.291605	7.238771	-0.087967	3.593959
457.815248	4406.240761	7.243776	-0.088081	3.597137
458.159015	4414.312419	7.248781	-0.088150	3.600354
458.422563	4422.354011	7.253786	-0.088204	3.603554
458.683526	4430.385739	7.258790	-0.088258	3.606747
459.106030	4438.402004	7.263795	-0.088342	3.609935
459.385884	4446.410587	7.268800	-0.088399	3.613114
459.665125	4454.504576	7.273805	-0.088457	3.616323
460.084110	4462.463096	7.278810	-0.088540	3.619480
460.856770	4470.452532	7.283814	-0.088689	3.622656
461.262228	4478.518263	7.288819	-0.088770	3.625850
461.496995	4486.519425	7.293824	-0.088818	3.629010
461.691680	4494.624902	7.298829	-0.088860	3.632207
462.386573	4502.587153	7.303834	-0.088994	3.635359
462.341773	4510.642140	7.308838	-0.088991	3.638524
462.957358	4518.643399	7.313843	-0.089111	3.641683
463.203361	4526.637997	7.318848	-0.089162	3.644827
463.608250	4534.686667	7.323853	-0.089243	3.647994
464.663098	4542.607121	7.328858	-0.089444	3.651125
464.359127	4550.726655	7.333862	-0.089393	3.654295
464.732173	4558.786220	7.338867	-0.089468	3.657456
464.733186	4566.805896	7.343872	-0.089473	3.660590
465.491008	4574.753093	7.348877	-0.089619	3.663712
465.144062	4582.935488	7.353882	-0.089560	3.666894
465.440322	4590.912451	7.358886	-0.089620	3.670011
466.012283	4598.877497	7.363891	-0.089732	3.673127
466.806655	4606.831207	7.368896	-0.089885	3.676242
467.440622	4614.835068	7.373901	-0.090008	3.679370
467.443236	4622.936247	7.378906	-0.090014	3.682516
467.441802	4630.996337	7.383910	-0.090019	3.685643
467.535618	4639.058476	7.388915	-0.090041	3.688771
468.172609	4647.021690	7.393920	-0.090165	3.691872
468.476318	4655.056171	7.398925	-0.090227	3.694989
468.711225	4663.077133	7.403930	-0.090276	3.698097
469.247642	4671.077610	7.408934	-0.090381	3.701202
469.474168	4679.112899	7.413939	-0.090428	3.704310
469.331113	4687.215937	7.418944	-0.090407	3.707431
470.171095	4695.177422	7.423949	-0.090569	3.710521
470.479960	4703.280628	7.428954	-0.090631	3.713649
470.854009	4711.248525	7.433958	-0.090706	3.716724
471.441828	4719.233592	7.438963	-0.090821	3.719808
471.635987	4727.234951	7.443968	-0.090862	3.722886
471.851022	4735.289688	7.448973	-0.090907	3.725982
472.147225	4743.297909	7.453978	-0.090968	3.729060
472.434700	4751.315080	7.458982	-0.091026	3.732139
473.171638	4759.360649	7.463987	-0.091169	3.735237
473.016599	4767.399454	7.468992	-0.091145	3.738308
473.640631	4775.397394	7.473997	-0.091266	3.741379
474.240038	4783.365318	7.479002	-0.091383	3.744436
474.166623	4791.481882	7.484006	-0.091375	3.747531
474.822972	4799.483475	7.489011	-0.091502	3.750597
475.544288	4807.426306	7.494016	-0.091642	3.753640
475.584127	4815.505848	7.499021	-0.091654	3.756716
475.911989	4823.495912	7.504026	-0.091720	3.759762
475.542904	4831.596265	7.509030	-0.091657	3.762831
476.347602	4839.578784	7.514035	-0.091812	3.765880
476.626954	4847.566251	7.519040	-0.091869	3.768917
477.672222	4855.544085	7.524045	-0.092069	3.771965
478.092358	4863.622761	7.529050	-0.092152	3.775034
477.691779	4871.724131	7.534054	-0.092083	3.778091
478.157873	4879.756329	7.539059	-0.092175	3.781138
478.512817	4887.688766	7.544064	-0.092246	3.784143
478.725584	4895.777838	7.549069	-0.092291	3.787202
479.462305	4903.765478	7.554074	-0.092433	3.790231
479.400283	4911.830672	7.559078	-0.092427	3.793269
479.368608	4919.937801	7.564083	-0.092426	3.796321
479.703607	4927.820165	7.569088	-0.092494	3.799295
480.506980	4935.821942	7.574093	-0.092649	3.802321
481.030717	4943.807293	7.579098	-0.092751	3.805333
480.780944	4951.921093	7.584102	-0.092710	3.808372
481.498518	4959.915441	7.589107	-0.092849	3.811387
481.608417	4967.918300	7.594112	-0.092875	3.814388
482.011770	4975.956884	7.599117	-0.092955	3.817407
482.419311	4983.981735	7.604122	-0.093036	3.820419
483.003970	4991.926683	7.609126	-0.093150	3.823402
483.461559	5000.008437	7.614131	-0.093240	3.826431
483.294320	5008.104787	7.619136	-0.093214	3.829449
483.851996	5016.094151	7.624141	-0.093323	3.832441
483.760786	5024.160275	7.629146	-0.093312	3.835445
484.401365	5032.071349	7.634150	-0.093436	3.838405
485.095045	5040.110830	7.639155	-0.093570	3.841411
485.238495	5048.154021	7.644160	-0.093602	3.844404
485.674240	5056.189373	7.649165	-0.093689	3.847398
485.606712	5064.255630	7.654170	-0.093681	3.850391
486.333582	5072.198861	7.659174	-0.093822	3.853353
486.528612	5080.340398	7.664179	-0.093863	3.856374
486.722292	5088.238852	7.669184	-0.093905	3.859303
487.392121	5096.296435	7.674189	-0.094035	3.862299
487.591772	5104.330288	7.679194	-0.094077	3.865273
487.278678	5112.406621	7.684198	-0.094024	3.868251
487.294092	5120.488561	7.689203	-0.094032	3.871235
488.364004	5128.476036	7.694208	-0.094236	3.874203
488.400182	5136.478842	7.699213	-0.094248	3.877154
488.991418	5144.430967	7.704218	-0.094363	3.880095
489.183952	5152.387467	7.709222	-0.094404	3.883027
489.666979	5160.447165	7.714227	-0.094500	3.886001
489.492029	5168.470848	7.719232	-0.094472	3.888946
490.160259	5176.521194	7.724237	-0.094602	3.891915
490.460554	5184.557845	7.729242	-0.094663	3.894870
490.291504	5192.557837	7.734246	-0.094637	3.897799
490.613399	5200.621011	7.739251	-0.094702	3.900760
491.039810	5208.538983	7.744256	-0.094786	3.903667
491.360056	5216.594207	7.749261	-0.094851	3.906619
491.559329	5224.631323	7.754266	-0.094893	3.909561
491.646982	5232.672785	7.759270	-0.094915	3.912500
492.295572	5240.675416	7.764275	-0.095041	3.915433
492.221070	5248.698265	7.769280	-0.095032	3.918357
493.150585	5256.693497	7.774285	-0.095210	3.921288
493.548901	5264.659290	7.779290	-0.095290	3.924197
493.415495	5272.729975	7.784294	-0.095270	3.927131
493.795215	5280.829111	7.789299	-0.095346	3.930083
494.151894	5288.789552	7.794304	-0.095418	3.932981
494.334241	5296.887122	7.799309	-0.095457	3.935924
494.767059	5304.875600	7.804314	-0.095543	3.938830
495.280211	5312.846268	7.809318	-0.095643	3.941729
495.412110	5320.881144	7.814323	-0.095673	3.944642
495.685097	5328.935612	7.819328	-0.095729	3.947562
495.880470	5336.979346	7.824333	-0.095771	3.950475
496.293217	5344.983658	7.829338	-0.095853	3.953375
496.764763	5352.985045	7.834342	-0.095946	3.956274
496.825361	5360.986961	7.839347	-0.095962	3.959162
497.438700	5369.001179	7.844352	-0.096082	3.962063
497.228416	5377.060402	7.849357	-0.096048	3.964964
497.728696	5385.041120	7.854362	-0.096146	3.967846
498.351825	5393.042688	7.859366	-0.096267	3.970736
498.738980	5401.083567	7.864371	-0.096344	3.973634
498.989575	5409.083216	7.869376	-0.096396	3.976513
499.149575	5417.098371	7.874381	-0.096431	3.979393
499.508582	5425.187313	7.879386	-0.096503	3.982301
499.945251	5433.138347	7.884390	-0.096590	3.985159
499.850510	5441.240078	7.889395	-0.096577	3.988060
500.895659	5449.146932	7.894400	-0.096777	3.990908
500.952185	5457.219301	7.899405	-0.096793	3.993796
500.797516	5465.317110	7.904410	-0.096769	3.996688
500.855222	5473.262116	7.909414	-0.096785	3.999527
501.294426	5481.327091	7.914419	-0.096872	4.002413
501.559231	5489.294118	7.919424	-0.096927	4.005259
501.685004	5497.327702	7.924429	-0.096955	4.008124
502.204967	5505.373456	7.929434	-0.097057	4.010999
502.247587	5513.362025	7.934438	-0.097070	4.013842
502.258106	5521.449960	7.939443	-0.097078	4.016719
502.505870	5529.450290	7.944448	-0.097129	4.019566
502.963453	5537.429296	7.949453	-0.097219	4.022407
503.286797	5545.422848	7.954458	-0.097285	4.025249
503.648850	5553.434543	7.959462	-0.097357	4.028096
504.275020	5561.495762	7.964467	-0.097479	4.030963
503.700249	5569.664157	7.969472	-0.097377	4.033846
504.518269	5577.568055	7.974477	-0.097535	4.036656
504.798894	5585.566031	7.979482	-0.097592	4.039489
504.713495	5593.588502	7.984486	-0.097581	4.042322
505.121547	5601.602035	7.989491	-0.097663	4.045158
505.750085	5609.555112	7.994496	-0.097785	4.047974
505.798599	5617.656089	7.999501	-0.097799	4.050832
505.736709	5625.713519	8.004506	-0.097793	4.053670
506.103179	5633.705821	8.009510	-0.097866	4.056490
506.880473	5641.643650	8.014515	-0.098016	4.059294
506.565146	5649.774209	8.019520	-0.097963	4.062149
506.917600	5657.744262	8.024525	-0.098033	4.064954
507.452528	5665.780757	8.029530	-0.098138	4.067784
508.088816	5673.750285	8.034534	-0.098262	4.070590
507.822946	5681.867543	8.039539	-0.098217	4.073432
507.986180	5689.871777	8.044544	-0.098253	4.076239
508.471151	5697.810293	8.049549	-0.098348	4.079026
508.759586	5705.882158	8.054554	-0.098407	4.081854
508.884094	5713.843222	8.059558	-0.098436	4.084640
509.010639	5721.910694	8.064563	-0.098465	4.087461
509.308062	5729.884726	8.069568	-0.098525	4.090249
509.268471	5737.978213	8.074573	-0.098523	4.093073
509.792147	5745.981152	8.079578	-0.098626	4.095871
510.809386	5753.883072	8.084582	-0.098820	4.098638
510.939676	5761.988474	8.089587	-0.098850	4.101462
511.240714	5769.917732	8.094592	-0.098911	4.104226
511.796427	5777.988807	8.099597	-0.099020	4.107040
512.104860	5786.080766	8.104602	-0.099082	4.109856
512.173492	5794.107742	8.109606	-0.099100	4.112644
512.777063	5802.083394	8.114611	-0.099218	4.115420
512.809584	5810.083186	8.119616	-0.099229	4.118194
513.154559	5818.153869	8.124621	-0.099298	4.120996
513.270884	5826.162298	8.129626	-0.099325	4.123771
513.386387	5834.196061	8.134630	-0.099352	4.126552
513.904202	5842.166766	8.139635	-0.099453	4.129316
514.607530	5850.144168	8.144640	-0.099590	4.132082
515.211220	5858.160797	8.149645	-0.099707	4.134858
515.366245	5866.235112	8.154650	-0.099741	4.137647
515.836506	5874.214499	8.159654	-0.099834	4.140405
515.548877	5882.320734	8.164659	-0.099786	4.143195
515.638733	5890.346818	8.169664	-0.099808	4.145960
516.132376	5898.307295	8.174669	-0.099905	4.148706
516.550338	5906.348646	8.179674	-0.099988	4.151477
516.676735	5914.308872	8.184678	-0.100016	4.154215
517.042787	5922.375805	8.189683	-0.100090	4.156991
517.547742	5930.323227	8.194688	-0.100189	4.159725
518.300803	5938.328270	8.199693	-0.100334	4.162480
518.445414	5946.398718	8.204698	-0.100366	4.165248
518.570350	5954.447032	8.209702	-0.100395	4.168007
518.948906	5962.519238	8.214707	-0.100471	4.170775
519.228420	5970.475350	8.219712	-0.100528	4.173500
519.693128	5978.514422	8.224717	-0.100620	4.176254
519.805580	5986.521750	8.229722	-0.100646	4.178991
519.101612	5994.656504	8.234726	-0.100520	4.181760
519.750104	6002.567338	8.239731	-0.100646	4.184467
519.983330	6010.619415	8.244736	-0.100694	4.187215
520.294923	6018.632095	8.249741	-0.100758	4.189949
520.207309	6026.763443	8.254746	-0.100747	4.192717
520.514094	6034.682390	8.259750	-0.100809	4.195416
521.108282	6042.674218	8.264755	-0.100925	4.198140
521.631881	6050.669212	8.269760	-0.101027	4.200863
521.885312	6058.622338	8.274765	-0.101080	4.203567
522.402210	6066.720295	8.279770	-0.101181	4.206321
522.538972	6074.683188	8.284774	-0.101212	4.209024
522.858940	6082.802943	8.289779	-0.101277	4.211780
523.263757	6090.722627	8.294784	-0.101357	4.214467
523.582397	6098.787724	8.299789	-0.101422	4.217200
523.888049	6106.805981	8.304794	-0.101484	4.219916
524.390071	6114.782757	8.309798	-0.101582	4.222618
524.837054	6122.796144	8.314803	-0.101671	4.225330
524.952231	6130.863030	8.319808	-0.101697	4.228055
524.721518	6138.935597	8.324813	-0.101660	4.230777
525.017504	6146.961112	8.329818	-0.101720	4.233486
525.060410	6154.972681	8.334822	-0.101733	4.236186
525.431979	6162.930354	8.339827	-0.101807	4.238870
525.519605	6170.994506	8.344832	-0.101829	4.241585
526.082755	6178.916975	8.349837	-0.101939	4.244255
526.667877	6186.999188	8.354842	-0.102053	4.246977
526.973716	6194.963921	8.359846	-0.102115	4.249656
527.284977	6203.056458	8.364851	-0.102178	4.252375
527.492208	6211.050258	8.369856	-0.102222	4.255059
528.650228	6218.939941	8.374861	-0.102443	4.257715
528.817622	6227.072990	8.379866	-0.102479	4.260442
528.940717	6235.033494	8.384870	-0.102507	4.263108
529.198969	6243.121240	8.389875	-0.102561	4.265817
529.249147	6251.135993	8.394880	-0.102575	4.268497
529.244512	6259.197515	8.399885	-0.102580	4.271191
529.952374	6267.151952	8.404890	-0.102717	4.273854
530.057370	6275.193615	8.409894	-0.102741	4.276539
529.901011	6283.205338	8.414899	-0.102717	4.279210
530.174832	6291.261017	8.419904	-0.102774	4.281898
530.715782	6299.163803	8.424909	-0.102879	4.284535
530.759095	6307.283760	8.429914	-0.102893	4.287239
531.326790	6315.195122	8.434918	-0.103004	4.289876
532.106151	6323.261033	8.439923	-0.103154	4.292565
532.025619	6331.285088	8.444928	-0.103144	4.295230
532.403143	6339.292903	8.449933	-0.103220	4.297893
532.820965	6347.359396	8.454938	-0.103303	4.300573
532.635975	6355.362580	8.459942	-0.103273	4.303226
533.074895	6363.419006	8.464947	-0.103360	4.305900
533.053706	6371.419518	8.469952	-0.103361	4.308550
533.854763	6379.439493	8.474957	-0.103516	4.311212
534.194742	6387.380746	8.479962	-0.103584	4.313842
534.217074	6395.447135	8.484966	-0.103594	4.316509
534.935096	6403.373168	8.489971	-0.103732	4.319133
535.094356	6411.465256	8.494976	-0.103767	4.321807
535.148855	6419.442843	8.499981	-0.103783	4.324440
535.614912	6427.500834	8.504986	-0.103875	4.327101
536.212141	6435.447214	8.509990	-0.103991	4.329725
536.316170	6443.510602	8.514995	-0.104016	4.332382
536.222512	6451.587331	8.520000	-0.104003	4.335040
537.119652	6459.490712	8.525005	-0.104175	4.337647
537.139069	6467.596684	8.530010	-0.104184	4.340312
537.328662	6475.525157	8.535014	-0.104225	4.342918
537.675630	6483.580514	8.540019	-0.104295	4.345566
537.613074	6491.663273	8.545024	-0.104288	4.348218
537.876830	6499.630518	8.550029	-0.104342	4.350833
538.508823	6507.719518	8.555034	-0.104465	4.353489
538.341967	6515.781267	8.560039	-0.104439	4.356129
538.834679	6523.738447	8.565043	-0.104536	4.358737
539.486288	6531.702028	8.570048	-0.104663	4.361347
539.689605	6539.646566	8.575053	-0.104706	4.363946
539.901025	6547.776384	8.580058	-0.104750	4.366604
539.779400	6555.729678	8.585063	-0.104733	4.369201
540.081788	6563.857042	8.590067	-0.104795	4.371856
540.312977	6571.847292	8.595072	-0.104843	4.374463
540.733471	6579.808952	8.600077	-0.104926	4.377062
540.981765	6587.882432	8.605082	-0.104978	4.379693
541.317672	6595.834479	8.610087	-0.105045	4.382285
541.489550	6603.869397	8.615091	-0.105083	4.384900
541.721164	6611.962787	8.620096	-0.105131	4.387534
542.085482	6619.941406	8.625101	-0.105204	4.390129
542.139105	6628.049928	8.630106	-0.105219	4.392763
542.271873	6636.031044	8.635111	-0.105249	4.395355
543.046602	6643.953205	8.640115	-0.105398	4.397929
543.364893	6651.982981	8.645120	-0.105463	4.400535
543.251397	6659.979119	8.650125	-0.105447	4.403125
543.405442	6668.093806	8.655130	-0.105481	4.405754
543.701681	6676.046881	8.660135	-0.105541	4.408329
543.575844	6684.215762	8.665139	-0.105523	4.410971
543.815495	6692.168772	8.670144	-0.105573	4.413543
544.122285	6700.191119	8.675149	-0.105635	4.416137
544.548035	6708.193109	8.680154	-0.105720	4.418722
544.938426	6716.177323	8.685159	-0.105797	4.421301
544.977407	6724.217615	8.690163	-0.105810	4.423894
545.578531	6732.248731	8.695168	-0.105927	4.426486
546.142667	6740.234008	8.700173	-0.106037	4.429061
546.232207	6748.349991	8.705178	-0.106059	4.431674
546.202179	6756.256205	8.710183	-0.106059	4.434217
545.931270	6764.405692	8.715187	-0.106013	4.436836
546.031743	6772.347269	8.720192	-0.106037	4.439389
546.448186	6780.328602	8.725197	-0.106120	4.441954
547.091173	6788.270513	8.730202	-0.106245	4.444506
547.225723	6796.341484	8.735207	-0.106275	4.447096
547.882012	6804.360043	8.740211	-0.106403	4.449670
547.832424	6812.465648	8.745216	-0.106399	4.452267
548.146851	6820.371937	8.750221	-0.106462	4.454800
548.420626	6828.470770	8.755226	-0.106518	4.457393
549.181605	6836.384260	8.760231	-0.106665	4.459928
549.358439	6844.454970	8.765235	-0.106703	4.462508
549.603527	6852.441555	8.770240	-0.106754	4.465061
549.984125	6860.469198	8.775245	-0.106830	4.467626
550.075845	6868.591433	8.780250	-0.106853	4.470218
550.320114	6876.542204	8.785255	-0.106903	4.472754
550.839799	6884.517688	8.790259	-0.107005	4.475298
550.974989	6892.555561	8.795264	-0.107035	4.477859
550.736754	6900.561386	8.800269	-0.106996	4.480407
551.183287	6908.553769	8.805274	-0.107085	4.482952
551.339066	6916.547386	8.810279	-0.107119	4.485495
551.597982	6924.625001	8.815283	-0.107172	4.488063
551.599918	6932.650269	8.820288	-0.107178	4.490612
552.059877	6940.623894	8.825293	-0.107269	4.493145
552.361041	6948.666925	8.830298	-0.107330	4.495698
552.462617	6956.652765	8.835303	-0.107354	4.498230
552.602796	6964.761985	8.840307	-0.107385	4.500801
553.028578	6972.664932	8.845312	-0.107470	4.503305
553.233850	6980.709829	8.850317	-0.107513	4.505852
553.656584	6988.779927	8.855322	-0.107597	4.508407
553.986194	6996.779626	8.860327	-0.107664	4.510937
554.363202	7004.815131	8.865331	-0.107739	4.513477
554.563386	7012.816418	8.870336	-0.107781	4.516005
555.088709	7020.738195	8.875341	-0.107884	4.518507
555.428072	7028.840457	8.880346	-0.107953	4.521064
555.810152	7036.714310	8.885351	-0.108029	4.523547
556.032520	7044.844741	8.890355	-0.108076	4.526110
556.506414	7052.804256	8.895360	-0.108169	4.528618
556.443943	7060.892773	8.900365	-0.108163	4.531164
556.462896	7068.936535	8.905370	-0.108171	4.533694
556.921236	7076.938710	8.910375	-0.108262	4.536211
557.126651	7084.912631	8.915379	-0.108305	4.538717
557.334346	7092.998429	8.920384	-0.108349	4.541257
557.535150	7100.912781	8.925389	-0.108392	4.543741
558.377953	7108.966483	8.930394	-0.108554	4.546269
558.661650	7116.910232	8.935399	-0.108612	4.548760
558.912177	7125.049033	8.940403	-0.108664	4.551311
559.199790	7132.981859	8.945408	-0.108722	4.553796
559.365991	7141.066554	8.950413	-0.108759	4.556327
559.689419	7149.021109	8.955418	-0.108824	4.558816
559.924345	7157.066557	8.960423	-0.108873	4.561331
560.103494	7165.029905	8.965427	-0.108911	4.563820
560.161504	7173.112324	8.970432	-0.108927	4.566344
560.500274	7181.084738	8.975437	-0.108996	4.568833
561.268562	7189.155618	8.980442	-0.109144	4.571352
561.239637	7197.105838	8.985447	-0.109144	4.573830
561.308277	7205.205244	8.990451	-0.109162	4.576354
561.627682	7213.156641	8.995456	-0.109226	4.578831
562.044259	7221.219427	9.000461	-0.109309	4.581341
562.281347	7229.186128	9.005466	-0.109358	4.583819
562.462380	7237.239817	9.010471	-0.109397	4.586323
562.900440	7245.242796	9.015475	-0.109484	4.588811
562.831856	7253.311340	9.020480	-0.109477	4.591316
563.345027	7261.246594	9.025485	-0.109577	4.593780
563.577333	7269.322048	9.030490	-0.109626	4.596285
563.887339	7277.278911	9.035495	-0.109689	4.598753
564.028213	7285.339375	9.040499	-0.109720	4.601251
564.290292	7293.261821	9.045504	-0.109774	4.603705
564.473794	7301.313874	9.050509	-0.109813	4.606197
564.522592	7309.363574	9.055514	-0.109828	4.608688
564.683281	7317.421491	9.060519	-0.109863	4.611179
565.182289	7325.391333	9.065523	-0.109961	4.613643
565.218002	7333.437072	9.070528	-0.109973	4.616128
565.293037	7341.385960	9.075533	-0.109992	4.618582
565.651656	7349.495701	9.080538	-0.110064	4.621084
565.772767	7357.379291	9.085543	-0.110091	4.623515
566.016018	7365.456480	9.090547	-0.110142	4.626004
566.328997	7373.477266	9.095552	-0.110205	4.628475
566.634452	7381.521742	9.100557	-0.110268	4.630952
566.913869	7389.490477	9.105562	-0.110325	4.633404
567.244514	7397.538699	9.110567	-0.110391	4.635879
567.555010	7405.535474	9.115571	-0.110454	4.638337
567.726215	7413.612785	9.120576	-0.110492	4.640818
567.712151	7421.538747	9.125581	-0.110494	4.643252
568.378529	7429.608911	9.130586	-0.110623	4.645728
568.431089	7437.571981	9.135591	-0.110638	4.648171
568.905720	7445.620301	9.140595	-0.110732	4.650638
569.264350	7453.637239	9.145600	-0.110804	4.653094
569.177284	7461.656778	9.150605	-0.110793	4.655550
569.288488	7469.691106	9.155610	-0.110819	4.658008
569.432810	7477.724696	9.160615	-0.110851	4.660466
569.900844	7485.726563	9.165619	-0.110943	4.662912
570.048586	7493.725890	9.170624	-0.110976	4.665356
570.030389	7501.724941	9.175629	-0.110978	4.667799
570.330469	7509.823224	9.180634	-0.111039	4.670271
570.541461	7517.835570	9.185639	-0.111083	4.672715
571.065471	7525.832744	9.190643	-0.111186	4.675153
571.437028	7533.838899	9.195648	-0.111260	4.677592
571.396488	7541.829417	9.200653	-0.111258	4.680026
571.494665	7549.843088	9.205658	-0.111281	4.682466
571.724365	7557.794807	9.210663	-0.111329	4.684885
572.054541	7565.902109	9.215667	-0.111396	4.687350
572.226984	7573.835372	9.220672	-0.111433	4.689761
572.580886	7581.885681	9.225677	-0.111504	4.692207
573.019111	7589.886234	9.230682	-0.111591	4.694635
572.924203	7598.005728	9.235687	-0.111579	4.697099
573.064859	7605.963902	9.240691	-0.111610	4.699513
573.417936	7614.025243	9.245696	-0.111681	4.701956
573.606457	7621.915817	9.250701	-0.111721	4.704347
573.566839	7630.091697	9.255706	-0.111719	4.706823
573.879156	7638.047016	9.260711	-0.111782	4.709230
574.175366	7646.128241	9.265715	-0.111843	4.711674
574.081457	7654.112133	9.270720	-0.111830	4.714089
573.665518	7662.185795	9.275725	-0.111758	4.716529
574.845996	7670.051035	9.280730	-0.111983	4.718903
575.332298	7678.073067	9.285735	-0.112079	4.721324
575.411574	7686.023001	9.290739	-0.112099	4.723722
575.952530	7694.103650	9.295744	-0.112205	4.726158
576.109128	7702.132930	9.300749	-0.112239	4.728578
576.241926	7710.225291	9.305754	-0.112269	4.731016
576.442704	7718.161678	9.310759	-0.112312	4.733405
576.820601	7726.242651	9.315763	-0.112387	4.735836
577.300237	7734.178250	9.320768	-0.112482	4.738222
577.637826	7742.248737	9.325773	-0.112550	4.740647
577.496104	7750.315135	9.330778	-0.112528	4.743071
578.093628	7758.282028	9.335783	-0.112645	4.745463
578.149111	7766.367844	9.340787	-0.112660	4.747890
578.495800	7774.323162	9.345792	-0.112730	4.750275
578.343992	7782.337216	9.350797	-0.112707	4.752679
578.998338	7790.387101	9.355802	-0.112834	4.755090
579.262446	7798.343630	9.360807	-0.112888	4.757473
579.548219	7806.382700	9.365811	-0.112947	4.759879
579.450767	7814.435558	9.370816	-0.112934	4.762289
579.831449	7822.334634	9.375821	-0.113010	4.764650
580.291870	7830.430840	9.380826	-0.113101	4.767069
580.354705	7838.437118	9.385831	-0.113118	4.769461
580.182357	7846.496068	9.390835	-0.113091	4.771869
580.304399	7854.502731	9.395840	-0.113119	4.774258
580.579445	7862.507894	9.400845	-0.113175	4.776646
580.692394	7870.462917	9.405850	-0.113201	4.779018
580.889064	7878.540287	9.410855	-0.113243	4.781424
581.112725	7886.465944	9.415859	-0.113290	4.783785
581.926223	7894.553891	9.420864	-0.113447	4.786190
582.086211	7902.542572	9.425869	-0.113482	4.788567
582.596632	7910.604832	9.430874	-0.113582	4.790963
582.740870	7918.542664	9.435879	-0.113614	4.793322
582.833248	7926.656145	9.440883	-0.113636	4.795732
582.907298	7934.602118	9.445888	-0.113655	4.798092
582.979810	7942.672997	9.450893	-0.113674	4.800488
583.434203	7950.635283	9.455898	-0.113764	4.802848
583.764767	7958.616799	9.460903	-0.113830	4.805214
583.688022	7966.696744	9.465907	-0.113821	4.807609
583.880357	7974.680178	9.470912	-0.113862	4.809973
584.074367	7982.768889	9.475917	-0.113904	4.812367
584.109897	7990.223142	9.480922	-0.113915	4.814573
584.327944	7995.052123	9.485927	-0.113959	4.816001

584.629173	7997.582439	9.490931	-0.114017	4.816748
584.523089	7999.014439	9.495936	-0.113998	4.817172
584.106136	7999.518147	9.500941	-0.113920	4.817323
584.734501	8000.245403	9.505946	-0.114038	4.817535
584.595916	8000.319353	9.510951	-0.114012	4.817558
584.694058	8000.214177	9.515955	-0.114030	4.817526
584.857862	8000.211334	9.520960	-0.114061	4.817525
585.155703	8000.445929	9.525965	-0.114116	4.817593
585.275638	8000.356913	9.530970	-0.114138	4.817566
585.120121	8000.403161	9.535975	-0.114109	4.817580
585.931387	8000.341335	9.540979	-0.114260	4.817558
585.889027	8000.318528	9.545984	-0.114252	4.817552
586.450273	8000.581344	9.550989	-0.114357	4.817627
586.442928	8000.494652	9.555994	-0.114356	4.817601
586.728235	8000.463003	9.560999	-0.114409	4.817591
586.870397	8000.565425	9.566003	-0.114435	4.817620
587.150407	8000.580155	9.571008	-0.114487	4.817624
587.065915	8000.469083	9.576013	-0.114471	4.817591
587.079991	8000.370040	9.581018	-0.114474	4.817562
586.849652	8000.416228	9.586023	-0.114431	4.817576
587.159862	8000.305761	9.591027	-0.114489	4.817542
587.386537	8000.364041	9.596032	-0.114531	4.817559
587.197000	8000.444625	9.601037	-0.114496	4.817583
587.667864	8000.497045	9.606042	-0.114583	4.817597
587.416639	8000.477458	9.611047	-0.114537	4.817592
587.726481	8000.427170	9.616051	-0.114594	4.817576
587.854454	8000.496651	9.621056	-0.114618	4.817596
587.530773	8000.399960	9.626061	-0.114558	4.817569
587.692221	8000.366465	9.631066	-0.114588	4.817558
587.699365	8000.391909	9.636071	-0.114589	4.817566
587.832845	8000.519545	9.641075	-0.114614	4.817603
588.010865	8000.407107	9.646080	-0.114647	4.817569
587.864263	8000.451376	9.651085	-0.114620	4.817582
587.968750	8000.464545	9.656090	-0.114639	4.817586
587.650869	8000.357383	9.661095	-0.114580	4.817556
587.992611	8000.384648	9.666099	-0.114643	4.817562
588.080152	8000.389118	9.671104	-0.114660	4.817563
588.106493	8000.408514	9.676109	-0.114664	4.817569
588.255480	8000.387503	9.681114	-0.114692	4.817562
588.382977	8000.368284	9.686119	-0.114716	4.817556
588.316857	8000.532013	9.691123	-0.114704	4.817604
588.107408	8000.313486	9.696128	-0.114664	4.817541
588.199399	8000.333861	9.701133	-0.114681	4.817546
588.523562	8000.338692	9.706138	-0.114742	4.817546
588.495113	8000.323482	9.711143	-0.114736	4.817542
588.313674	8000.320773	9.716147	-0.114703	4.817542
588.008076	8000.207459	9.721152	-0.114646	4.817510
588.489827	8000.352958	9.726157	-0.114735	4.817551
589.071906	8000.352135	9.731162	-0.114844	4.817548
588.625333	8000.366588	9.736167	-0.114761	4.817554
588.973622	8000.514327	9.741171	-0.114825	4.817596
588.745304	8000.297627	9.746176	-0.114783	4.817533
588.794713	8000.388111	9.751181	-0.114792	4.817560
588.853085	8000.387923	9.756186	-0.114803	4.817559
588.655196	8000.249815	9.761191	-0.114766	4.817519
589.241893	8000.411668	9.766195	-0.114875	4.817565
589.403358	8000.508050	9.771200	-0.114905	4.817592
588.853608	8000.225311	9.776205	-0.114803	4.817511
589.052495	8000.363429	9.781210	-0.114840	4.817551
588.826836	8000.195341	9.786215	-0.114798	4.817502
589.283053	8000.255993	9.791219	-0.114882	4.817518
589.332836	8000.344372	9.796224	-0.114892	4.817544
589.169648	8000.232121	9.801229	-0.114861	4.817512
588.881395	8000.267942	9.806234	-0.114808	4.817524
588.910664	8000.139558	9.811239	-0.114813	4.817486
589.093706	8000.283774	9.816243	-0.114847	4.817527
589.172111	8000.099104	9.821248	-0.114861	4.817473
589.833861	8000.404626	9.826253	-0.114985	4.817560
589.501948	8000.085011	9.831258	-0.114923	4.817467
589.719655	8000.280429	9.836263	-0.114963	4.817524
589.759014	8000.248280	9.841267	-0.114971	4.817514
589.696129	8000.191376	9.846272	-0.114959	4.817497
589.481140	8000.358165	9.851277	-0.114919	4.817548
589.504085	8000.165275	9.856282	-0.114923	4.817491
589.623823	8000.371903	9.861287	-0.114945	4.817551
589.815560	8000.202648	9.866291	-0.114981	4.817500
589.910020	8000.370889	9.871296	-0.114999	4.817550
590.287342	8000.502174	9.876301	-0.115069	4.817587
590.212876	8000.310991	9.881306	-0.115055	4.817531
590.194077	8000.502887	9.886311	-0.115052	4.817587
590.090551	8000.410528	9.891315	-0.115032	4.817561
589.899287	8000.355930	9.896320	-0.114996	4.817545
589.928819	8000.346864	9.901325	-0.115002	4.817542
590.175430	8000.398059	9.906330	-0.115048	4.817556
590.064044	8000.350988	9.911335	-0.115027	4.817543
590.506937	8000.490644	9.916339	-0.115110	4.817582
590.254341	8000.428793	9.921344	-0.115062	4.817565
590.308388	8000.376800	9.926349	-0.115072	4.817550
590.227659	8000.313292	9.931354	-0.115057	4.817531
590.354596	8000.394379	9.936359	-0.115081	4.817555
590.228557	8000.401997	9.941363	-0.115057	4.817557
590.195224	8000.225158	9.946368	-0.115051	4.817505
590.689981	8000.472237	9.951373	-0.115143	4.817576
590.227441	8000.362902	9.956378	-0.115057	4.817546
590.209240	8000.458717	9.961383	-0.115054	4.817574
590.024627	8000.195146	9.966387	-0.115019	4.817497
590.058097	8000.348750	9.971392	-0.115025	4.817542
589.971100	8000.219682	9.976397	-0.115009	4.817505
590.254971	8000.284103	9.981402	-0.115062	4.817522
590.448083	8000.320772	9.986407	-0.115098	4.817532
590.441026	8000.406194	9.991411	-0.115097	4.817558
590.515469	8000.335498	9.996416	-0.115110	4.817537
589.925994	8000.174645	10.001421	-0.115001	4.817492
589.968701	8000.174224	10.006426	-0.115008	4.817491
590.250533	8000.267123	10.011431	-0.115061	4.817517
590.347789	8000.265404	10.016435	-0.115079	4.817517
590.312320	8000.264871	10.021440	-0.115072	4.817517
590.754521	8000.497440	10.026445	-0.115155	4.817583
590.842117	8000.396318	10.031450	-0.115171	4.817553
590.581006	8000.387136	10.036455	-0.115122	4.817551
590.679906	8000.514267	10.041459	-0.115141	4.817589
590.482555	8000.177643	10.046464	-0.115104	4.817490
590.270092	8000.176581	10.051469	-0.115064	4.817491
590.184847	8000.145740	10.056474	-0.115048	4.817482
590.273942	8000.260049	10.061479	-0.115065	4.817515
589.933938	8000.111369	10.066483	-0.115001	4.817473
589.904834	8000.088757	10.071488	-0.114996	4.817466
590.043081	8000.097152	10.076493	-0.115022	4.817468
590.276130	8000.085843	10.081498	-0.115065	4.817464
590.647490	8000.378594	10.086503	-0.115134	4.817549
590.319076	8000.226915	10.091507	-0.115073	4.817505
590.634956	8000.128146	10.096512	-0.115132	4.817475
590.462765	8000.132964	10.101517	-0.115100	4.817477
590.273562	8000.162871	10.106522	-0.115064	4.817487
590.415745	8000.154430	10.111527	-0.115091	4.817483
590.533974	8000.163583	10.116531	-0.115113	4.817486
590.723441	8000.283616	10.121536	-0.115148	4.817520
590.459066	8000.353581	10.126541	-0.115099	4.817542
590.922289	8000.164090	10.131546	-0.115185	4.817484
590.464961	8000.122416	10.136551	-0.115100	4.817474
590.806237	8000.103219	10.141555	-0.115163	4.817467
590.926802	8000.313035	10.146560	-0.115186	4.817528
590.499981	8000.238024	10.151565	-0.115106	4.817508
590.633160	8000.062614	10.156570	-0.115131	4.817455
590.540429	8000.179490	10.161575	-0.115114	4.817490
590.898059	8000.398124	10.166579	-0.115180	4.817553
590.991168	8000.218945	10.171584	-0.115198	4.817500
591.257656	8000.399264	10.176589	-0.115247	4.817552
591.116326	8000.164843	10.181594	-0.115221	4.817483
591.132546	8000.396333	10.186599	-0.115224	4.817552
590.892135	8000.236461	10.191603	-0.115179	4.817506
591.372154	8000.308038	10.196608	-0.115268	4.817525
591.002006	8000.358472	10.201613	-0.115199	4.817541
591.138057	8000.305592	10.206618	-0.115225	4.817525
591.414152	8000.376236	10.211623	-0.115276	4.817545
591.546021	8000.380315	10.216627	-0.115301	4.817545
591.467867	8000.389704	10.221632	-0.115286	4.817548
590.899728	8000.225993	10.226637	-0.115180	4.817502
591.574875	8000.191720	10.231642	-0.115306	4.817489
591.072832	8000.201117	10.236647	-0.115212	4.817494
590.812400	8000.237351	10.241651	-0.115164	4.817506
590.866226	8000.278277	10.246656	-0.115174	4.817518
590.886496	8000.086397	10.251661	-0.115177	4.817461
590.917731	8000.144936	10.256666	-0.115183	4.817478
591.291810	8000.334252	10.261671	-0.115253	4.817533
591.672740	8000.213223	10.266675	-0.115324	4.817495
591.757669	8000.140571	10.271680	-0.115339	4.817473
591.560774	8000.377329	10.276685	-0.115303	4.817544
591.623656	8000.405721	10.281690	-0.115315	4.817552
591.746861	8000.370599	10.286695	-0.115337	4.817542
591.488221	8000.388908	10.291699	-0.115289	4.817548
591.780003	8000.363696	10.296704	-0.115344	4.817539
591.853153	8000.512621	10.301709	-0.115357	4.817583
591.819386	8000.429748	10.306714	-0.115351	4.817559
591.908341	8000.329701	10.311719	-0.115367	4.817529
591.830414	8000.423571	10.316723	-0.115353	4.817557
591.725617	8000.350196	10.321728	-0.115333	4.817536
591.630116	8000.435356	10.326733	-0.115315	4.817561
591.773944	8000.211525	10.331738	-0.115342	4.817494
591.825455	8000.345342	10.336743	-0.115352	4.817534
591.327617	8000.171064	10.341747	-0.115259	4.817484
591.914552	8000.219951	10.346752	-0.115368	4.817496
591.774928	8000.246374	10.351757	-0.115342	4.817505
591.771295	8000.297002	10.356762	-0.115341	4.817520
591.100916	8000.122262	10.361767	-0.115216	4.817471
591.389863	8000.308195	10.366771	-0.115270	4.817525
591.984137	8000.431112	10.371776	-0.115381	4.817558
591.210092	8000.143945	10.376781	-0.115237	4.817477
591.335999	8000.219738	10.381786	-0.115260	4.817499
591.284115	8000.043674	10.386791	-0.115250	4.817447
591.007844	8000.129301	10.391795	-0.115199	4.817473
591.201665	8000.127968	10.396800	-0.115235	4.817472
591.725607	8000.315299	10.401805	-0.115333	4.817525
592.071496	8000.190579	10.406810	-0.115397	4.817487
591.748694	8000.157244	10.411815	-0.115337	4.817478
591.747608	8000.198407	10.416819	-0.115336	4.817491
591.924440	8000.215828	10.421824	-0.115369	4.817495
591.626951	8000.270516	10.426829	-0.115314	4.817512
591.819918	8000.154071	10.431834	-0.115350	4.817477
591.554249	8000.069850	10.436839	-0.115300	4.817453
591.195557	8000.050765	10.441843	-0.115233	4.817449
591.671934	8000.114894	10.446848	-0.115322	4.817466
591.885867	8000.190946	10.451853	-0.115362	4.817488
592.053217	8000.327550	10.456858	-0.115393	4.817527
592.104471	8000.325144	10.461863	-0.115403	4.817527
591.825353	8000.191089	10.466867	-0.115351	4.817488
592.345186	8000.399485	10.471872	-0.115447	4.817547
591.928674	8000.223248	10.476877	-0.115370	4.817497
592.027838	8000.290196	10.481882	-0.115388	4.817517
592.025585	8000.260592	10.486887	-0.115388	4.817508
592.008754	8000.354319	10.491891	-0.115385	4.817536
592.014450	8000.314274	10.496896	-0.115386	4.817524
591.806264	8000.318553	10.501901	-0.115347	4.817526
592.102538	8000.312415	10.506906	-0.115402	4.817523
592.463944	8000.530064	10.511911	-0.115469	4.817586
592.337962	8000.236728	10.516915	-0.115446	4.817499
592.400169	8000.293621	10.521920	-0.115457	4.817516
592.352771	8000.243279	10.526925	-0.115448	4.817501
592.133642	8000.245282	10.531930	-0.115407	4.817503
592.076230	8000.376418	10.536935	-0.115397	4.817542
591.916608	8000.352910	10.541939	-0.115367	4.817536
592.040005	8000.262882	10.546944	-0.115390	4.817508
592.283596	8000.323540	10.551949	-0.115435	4.817525
592.541033	8000.530132	10.556954	-0.115483	4.817585
592.252061	8000.322006	10.561959	-0.115429	4.817525
592.320365	8000.208979	10.566963	-0.115442	4.817491
592.507997	8000.239234	10.571968	-0.115477	4.817499
592.326233	8000.389631	10.576973	-0.115443	4.817545
592.495966	8000.354149	10.581978	-0.115475	4.817533
592.510997	8000.356483	10.586983	-0.115477	4.817534
592.160263	8000.279433	10.591987	-0.115412	4.817513
592.140370	8000.185152	10.596992	-0.115408	4.817485
592.101395	8000.302835	10.601997	-0.115401	4.817520
592.367495	8000.235001	10.607002	-0.115450	4.817499
592.315209	8000.188810	10.612007	-0.115441	4.817485
592.440251	8000.332175	10.617011	-0.115464	4.817527
592.330117	8000.241825	10.622016	-0.115443	4.817501
592.335684	8000.253520	10.627021	-0.115444	4.817504
592.470498	8000.329450	10.632026	-0.115469	4.817526
592.444071	8000.320604	10.637031	-0.115464	4.817524
592.514985	8000.269917	10.642035	-0.115478	4.817508
592.560888	8000.374086	10.647040	-0.115486	4.817539
592.483775	8000.400386	10.652045	-0.115472	4.817547
592.516038	8000.194949	10.657050	-0.115478	4.817486
592.901595	8000.368608	10.662055	-0.115549	4.817536
592.762808	8000.515426	10.667059	-0.115524	4.817580
593.023298	8000.373589	10.672064	-0.115572	4.817537
592.954694	8000.633393	10.677069	-0.115559	4.817614
592.754283	8000.242844	10.682074	-0.115522	4.817499
592.492023	8000.247370	10.687079	-0.115473	4.817502
592.294167	8000.339449	10.692083	-0.115436	4.817530
592.522320	8000.319623	10.697088	-0.115479	4.817523
592.326760	8000.279739	10.702093	-0.115442	4.817512
592.875323	8000.214013	10.707098	-0.115544	4.817490
592.629677	8000.322274	10.712103	-0.115498	4.817523
592.520153	8000.416728	10.717107	-0.115478	4.817552
592.361591	8000.135579	10.722112	-0.115448	4.817469
592.877331	8000.375596	10.727117	-0.115544	4.817538
592.909075	8000.273637	10.732122	-0.115550	4.817508
592.404217	8000.293546	10.737127	-0.115456	4.817516
592.606099	8000.264879	10.742131	-0.115494	4.817507
592.213324	8000.148132	10.747136	-0.115421	4.817474
591.956969	8000.052433	10.752141	-0.115373	4.817447
592.474352	8000.107674	10.757146	-0.115469	4.817461
592.584339	8000.195903	10.762151	-0.115490	4.817486
592.817497	8000.108570	10.767155	-0.115533	4.817459
592.499060	8000.115426	10.772160	-0.115474	4.817463
592.201545	8000.237694	10.777165	-0.115418	4.817500
592.297333	8000.131414	10.782170	-0.115436	4.817468
592.488641	8000.174395	10.787175	-0.115471	4.817480
592.631059	8000.398275	10.792179	-0.115498	4.817546
592.853096	8000.344566	10.797184	-0.115539	4.817529
592.719905	8000.344685	10.802189	-0.115515	4.817530
592.526628	8000.221412	10.807194	-0.115478	4.817494
592.512885	8000.181077	10.812199	-0.115476	4.817482
592.219843	8000.162969	10.817203	-0.115421	4.817478
592.655819	8000.183206	10.822208	-0.115502	4.817482
592.797995	8000.266637	10.827213	-0.115529	4.817506
592.698914	8000.221858	10.832218	-0.115510	4.817493
593.107966	8000.389534	10.837223	-0.115587	4.817541
593.255551	8000.244953	10.842227	-0.115614	4.817498
593.215985	8000.366854	10.847232	-0.115607	4.817534
592.820599	8000.427469	10.852237	-0.115533	4.817554
592.879876	8000.168579	10.857242	-0.115544	4.817477
593.012733	8000.324735	10.862247	-0.115569	4.817522
592.837695	8000.334788	10.867251	-0.115536	4.817526
592.993003	8000.244179	10.872256	-0.115565	4.817499
593.119927	8000.284088	10.877261	-0.115588	4.817510
592.859965	8000.036269	10.882266	-0.115540	4.817438
592.878185	8000.220278	10.887271	-0.115543	4.817492
593.100569	8000.217262	10.892275	-0.115585	4.817490
593.078851	8000.179975	10.897280	-0.115581	4.817479
593.107726	8000.269106	10.902285	-0.115586	4.817506
593.326732	8000.228024	10.907290	-0.115627	4.817492
593.078490	8000.209528	10.912295	-0.115580	4.817488
593.096599	8000.230915	10.917299	-0.115584	4.817494
593.297455	8000.285657	10.922304	-0.115621	4.817510
592.856053	8000.379376	10.927309	-0.115539	4.817539
592.822688	8000.062080	10.932314	-0.115532	4.817446
592.732498	8000.246581	10.937319	-0.115516	4.817501
592.761608	8000.253349	10.942323	-0.115521	4.817502
592.670177	8000.133711	10.947328	-0.115504	4.817468
592.516523	8000.306704	10.952333	-0.115475	4.817519
592.770213	8000.071840	10.957338	-0.115523	4.817449
592.801608	8000.129329	10.962343	-0.115528	4.817466
592.763798	8000.258646	10.967347	-0.115521	4.817504
592.681065	8000.153921	10.972352	-0.115506	4.817473
592.970476	8000.416959	10.977357	-0.115560	4.817550
592.729413	8000.158861	10.982362	-0.115515	4.817475
592.044441	8000.036696	10.987367	-0.115387	4.817442
592.221241	8000.018214	10.992371	-0.115420	4.817435
592.277668	7999.945136	10.997376	-0.115430	4.817414
592.446004	8000.039515	11.002381	-0.115462	4.817441
592.772788	7999.998986	11.007386	-0.115523	4.817427
592.776992	8000.160609	11.012391	-0.115523	4.817475
592.178062	8000.021777	11.017395	-0.115412	4.817437
592.316176	8000.082970	11.022400	-0.115437	4.817454
591.962675	8000.048121	11.027405	-0.115372	4.817445
591.980976	7999.939629	11.032410	-0.115375	4.817413
592.511843	8000.273845	11.037415	-0.115474	4.817510
592.311518	8000.053321	11.042419	-0.115436	4.817445
592.793754	7999.985546	11.047424	-0.115526	4.817423
592.528225	8000.115685	11.052429	-0.115477	4.817463
592.429683	7999.976935	11.057434	-0.115458	4.817422
592.218956	7999.988569	11.062439	-0.115419	4.817427
591.886117	7999.963533	11.067443	-0.115357	4.817421
592.141807	7999.935669	11.072448	-0.115405	4.817411
592.266399	7999.968149	11.077453	-0.115428	4.817420
592.977347	8000.109703	11.082458	-0.115560	4.817459
592.871898	8000.102845	11.087463	-0.115540	4.817458
592.786148	8000.156471	11.092467	-0.115524	4.817474
593.131582	8000.132061	11.097472	-0.115589	4.817465
592.654292	8000.104864	11.102477	-0.115500	4.817459
592.635245	7999.948294	11.107482	-0.115496	4.817413
592.646378	8000.136419	11.112487	-0.115498	4.817468
592.535695	8000.083020	11.117491	-0.115478	4.817453
592.662051	7999.985644	11.122496	-0.115501	4.817424
592.817393	8000.154804	11.127501	-0.115530	4.817473
592.839586	8000.042143	11.132506	-0.115534	4.817440
592.414922	8000.263886	11.137511	-0.115455	4.817507
592.586763	8000.150293	11.142515	-0.115487	4.817473
592.870548	8000.119682	11.147520	-0.115540	4.817463
592.707890	8000.080290	11.152525	-0.115509	4.817452
592.975119	8000.153973	11.157530	-0.115559	4.817472
592.729442	8000.076382	11.162535	-0.115513	4.817450
592.613781	8000.097883	11.167539	-0.115492	4.817457
592.692311	8000.027247	11.172544	-0.115506	4.817436
592.904565	8000.148683	11.177549	-0.115546	4.817471
592.855931	8000.256719	11.182554	-0.115537	4.817503
592.946881	8000.155645	11.187559	-0.115554	4.817473
593.021399	8000.362672	11.192563	-0.115568	4.817534
593.406496	8000.203689	11.197568	-0.115639	4.817485
593.697594	8000.523784	11.202573	-0.115694	4.817578
593.345859	8000.238681	11.207578	-0.115628	4.817496
592.995013	8000.268282	11.212583	-0.115563	4.817506
593.073964	8000.242003	11.217587	-0.115577	4.817498
592.940706	8000.006638	11.222592	-0.115552	4.817429
592.859920	8000.169104	11.227597	-0.115537	4.817477
592.446851	7999.907388	11.232602	-0.115460	4.817402
592.102153	7999.902239	11.237607	-0.115396	4.817402
592.311882	7999.951828	11.242611	-0.115435	4.817415
592.670658	7999.857923	11.247616	-0.115502	4.817386
592.980975	8000.150833	11.252621	-0.115559	4.817471
592.984485	8000.181506	11.257626	-0.115560	4.817480
593.122189	8000.195176	11.262631	-0.115586	4.817484
593.128671	8000.244901	11.267635	-0.115587	4.817498
593.337796	8000.167768	11.272640	-0.115626	4.817475
593.069194	8000.113064	11.277645	-0.115576	4.817460
593.214268	8000.071933	11.282650	-0.115603	4.817447
593.272361	8000.091806	11.287655	-0.115613	4.817453
592.881758	8000.088079	11.292659	-0.115541	4.817453
593.218586	8000.187090	11.297664	-0.115603	4.817481
592.931293	8000.113100	11.302669	-0.115550	4.817460
592.759978	7999.942639	11.307674	-0.115518	4.817411
593.080922	8000.103713	11.312679	-0.115578	4.817457
592.750971	8000.061822	11.317683	-0.115516	4.817446
593.009275	8000.005487	11.322688	-0.115564	4.817428
592.730326	8000.137537	11.327693	-0.115512	4.817468
593.053805	7999.993474	11.332698	-0.115572	4.817424
592.870400	8000.118504	11.337703	-0.115538	4.817462
592.807790	7999.938051	11.342707	-0.115526	4.817409
593.236078	8000.103897	11.347712	-0.115606	4.817456
593.001109	8000.050753	11.352717	-0.115562	4.817442
592.907005	8000.081023	11.357722	-0.115545	4.817451
592.685701	7999.956279	11.362727	-0.115504	4.817415
592.987125	8000.050535	11.367731	-0.115560	4.817442
592.848090	8000.013608	11.372736	-0.115534	4.817431
592.668961	8000.114414	11.377741	-0.115500	4.817462
593.093945	7999.951804	11.382746	-0.115579	4.817412
593.358086	8000.114143	11.387751	-0.115629	4.817459
593.274652	8000.060094	11.392755	-0.115613	4.817443
593.480825	8000.002980	11.397760	-0.115651	4.817425
593.483242	8000.121284	11.402765	-0.115652	4.817460
593.385063	8000.267652	11.407770	-0.115634	4.817504
592.685194	7999.910834	11.412775	-0.115503	4.817402
593.084528	8000.025559	11.417779	-0.115577	4.817434
593.198346	7999.977625	11.422784	-0.115599	4.817419
593.338617	8000.141283	11.427789	-0.115625	4.817467
593.543621	8000.148567	11.432794	-0.115663	4.817468
592.890260	7999.992021	11.437799	-0.115541	4.817425
592.613946	7999.955157	11.442803	-0.115490	4.817415
592.832597	7999.850711	11.447808	-0.115530	4.817383
592.896834	8000.106155	11.452813	-0.115542	4.817458
592.899847	7999.919290	11.457818	-0.115543	4.817403
593.587220	8000.179823	11.462823	-0.115671	4.817477
593.189765	8000.097850	11.467827	-0.115597	4.817455
593.377207	7999.958090	11.472832	-0.115631	4.817413
592.984417	8000.010298	11.477837	-0.115558	4.817430
593.244490	7999.912806	11.482842	-0.115607	4.817400
593.208448	8000.075941	11.487847	-0.115600	4.817448
593.180158	8000.000541	11.492851	-0.115595	4.817426
593.313885	7999.952904	11.497856	-0.115619	4.817411
592.869910	8000.003292	11.502861	-0.115537	4.817428
592.823627	7999.858987	11.507866	-0.115528	4.817386
592.666818	7999.870370	11.512871	-0.115499	4.817390
592.988182	7999.971258	11.517875	-0.115559	4.817418
592.971153	7999.836893	11.522880	-0.115555	4.817379
592.924164	7999.998807	11.527885	-0.115547	4.817427
593.250367	7999.929758	11.532890	-0.115607	4.817405
593.472393	8000.043949	11.537895	-0.115649	4.817438
592.753341	7999.973015	11.542899	-0.115515	4.817420
592.878937	7999.853452	11.547904	-0.115538	4.817384
593.241614	8000.052108	11.552909	-0.115606	4.817441
592.725922	7999.814203	11.557914	-0.115509	4.817373
593.154112	7999.963148	11.562919	-0.115589	4.817415
593.022285	7999.932665	11.567923	-0.115565	4.817407
592.959621	7999.797619	11.572928	-0.115553	4.817367
592.995831	7999.976614	11.577933	-0.115560	4.817420
593.428875	7999.966184	11.582938	-0.115640	4.817415
593.319581	8000.009955	11.587943	-0.115620	4.817428
592.724327	7999.973606	11.592947	-0.115509	4.817420
593.404470	7999.934131	11.597952	-0.115635	4.817405
593.427853	8000.065419	11.602957	-0.115640	4.817444
593.829283	8000.180182	11.607962	-0.115715	4.817476
593.836916	8000.200357	11.612967	-0.115716	4.817482
593.679216	8000.046989	11.617971	-0.115687	4.817438
593.425074	7999.962934	11.622976	-0.115639	4.817414
593.507537	7999.981059	11.627981	-0.115654	4.817419
593.523170	8000.140743	11.632986	-0.115657	4.817466
593.577004	8000.014826	11.637991	-0.115667	4.817428
593.394153	7999.966684	11.642995	-0.115633	4.817415
593.004049	7999.895384	11.648000	-0.115561	4.817396
593.109138	7999.990931	11.653005	-0.115580	4.817423
593.321356	7999.972979	11.658010	-0.115620	4.817417
593.109179	7999.920176	11.663015	-0.115580	4.817403
593.379097	8000.048809	11.668019	-0.115630	4.817439
593.570615	7999.837304	11.673024	-0.115666	4.817376
593.470004	7999.975187	11.678029	-0.115647	4.817417
592.955910	7999.984400	11.683034	-0.115551	4.817422
593.576801	8000.062311	11.688039	-0.115667	4.817443
593.450566	8000.050917	11.693043	-0.115643	4.817440
593.158974	7999.888162	11.698048	-0.115589	4.817393
593.429974	7999.947117	11.703053	-0.115639	4.817409
593.399308	7999.981503	11.708058	-0.115634	4.817419
593.340045	7999.997511	11.713063	-0.115623	4.817424
593.354212	7999.992439	11.718067	-0.115625	4.817423
593.483502	7999.984864	11.723072	-0.115649	4.817420
593.649424	8000.065482	11.728077	-0.115680	4.817443
593.764787	8000.024963	11.733082	-0.115702	4.817431
593.852278	8000.073787	11.738087	-0.115718	4.817445
593.872319	8000.141668	11.743091	-0.115722	4.817465
593.798246	7999.957871	11.748096	-0.115708	4.817411
593.981284	8000.163354	11.753101	-0.115742	4.817471
594.052994	8000.079942	11.758106	-0.115755	4.817446
593.717587	8000.040079	11.763111	-0.115693	4.817435
593.525067	7999.954833	11.768115	-0.115657	4.817411
594.197775	8000.093713	11.773120	-0.115782	4.817449
593.911539	8000.047192	11.778125	-0.115729	4.817437
593.958887	7999.903226	11.783130	-0.115737	4.817394
593.985630	7999.957477	11.788135	-0.115742	4.817410
593.996891	8000.079082	11.793139	-0.115744	4.817446
593.970390	7999.941403	11.798144	-0.115739	4.817405
593.789889	7999.985167	11.803149	-0.115706	4.817419
593.967373	7999.950856	11.808154	-0.115739	4.817408
593.811862	7999.950641	11.813159	-0.115710	4.817409
593.889028	8000.104910	11.818163	-0.115724	4.817454
593.988167	7999.939541	11.823168	-0.115742	4.817404
593.869441	8000.222883	11.828173	-0.115720	4.817489
593.588180	7999.937783	11.833178	-0.115668	4.817406
593.180518	7999.912683	11.838183	-0.115592	4.817400
593.471954	7999.941320	11.843187	-0.115646	4.817407
593.456380	7999.930525	11.848192	-0.115643	4.817404
593.373335	7999.884930	11.853197	-0.115628	4.817391
593.893269	7999.929653	11.858202	-0.115724	4.817402
593.894250	7999.979296	11.863207	-0.115725	4.817417
593.377018	7999.956782	11.868211	-0.115628	4.817412
593.649007	7999.957674	11.873216	-0.115679	4.817411
594.126179	8000.064065	11.878221	-0.115768	4.817441
593.680153	7999.997205	11.883226	-0.115685	4.817423
593.497548	7999.863532	11.888231	-0.115651	4.817384
593.558470	7999.973205	11.893235	-0.115662	4.817416
593.601023	7999.896751	11.898240	-0.115670	4.817394
593.722912	8000.072806	11.903245	-0.115692	4.817445
593.826890	8000.021557	11.908250	-0.115712	4.817429
594.065256	8000.227869	11.913255	-0.115756	4.817489
593.877168	8000.074046	11.918259	-0.115721	4.817445
594.140387	7999.945977	11.923264	-0.115770	4.817406
593.997859	7999.963908	11.928269	-0.115743	4.817412
593.871444	7999.929280	11.933274	-0.115720	4.817402
593.834822	8000.108248	11.938279	-0.115713	4.817455
593.792501	8000.194204	11.943283	-0.115705	4.817481
593.732359	7999.967320	11.948288	-0.115694	4.817414
593.556824	7999.909783	11.953293	-0.115661	4.817398
593.862972	8000.031569	11.958298	-0.115718	4.817432
594.368485	7999.959920	11.963303	-0.115812	4.817409
594.123260	8000.097756	11.968307	-0.115767	4.817451
593.927111	7999.866727	11.973312	-0.115730	4.817383
594.329768	7999.989956	11.978317	-0.115805	4.817418
594.034544	8000.041509	11.983322	-0.115750	4.817434
593.949576	7999.916685	11.988327	-0.115734	4.817398
593.957258	7999.862941	11.993331	-0.115735	4.817382
594.048439	8000.010027	11.998336	-0.115752	4.817425
594.159942	8000.099338	12.003341	-0.115773	4.817451
594.195118	8000.079797	12.008346	-0.115780	4.817445
593.884838	7999.971669	12.013351	-0.115722	4.817414
593.804873	8000.094022	12.018355	-0.115707	4.817451
593.748352	7999.895705	12.023360	-0.115696	4.817393
593.521929	7999.975742	12.028365	-0.115654	4.817417
593.872293	7999.994701	12.033370	-0.115719	4.817421
594.114814	8000.136658	12.038375	-0.115764	4.817462
594.536654	8000.243283	12.043379	-0.115843	4.817492
594.335887	7999.999507	12.048384	-0.115805	4.817421
594.185501	8000.136649	12.053389	-0.115777	4.817462
594.352373	8000.215173	12.058394	-0.115809	4.817484
594.286212	8000.031492	12.063399	-0.115796	4.817430
593.991097	8000.111558	12.068403	-0.115741	4.817455
593.716578	7999.951166	12.073408	-0.115690	4.817409
594.094737	8000.142669	12.078413	-0.115760	4.817464
594.061736	8000.020732	12.083418	-0.115754	4.817428
594.390764	8000.267473	12.088423	-0.115816	4.817500
594.346301	8000.096787	12.093427	-0.115807	4.817449
594.207781	8000.107386	12.098432	-0.115781	4.817453
594.660136	8000.268324	12.103437	-0.115866	4.817499
594.641546	8000.115976	12.108442	-0.115862	4.817454
594.299798	8000.121424	12.113447	-0.115798	4.817457
594.129163	8000.115702	12.118451	-0.115766	4.817456
594.411948	7999.996373	12.123456	-0.115819	4.817419
594.320142	8000.103766	12.128461	-0.115802	4.817452
594.255388	8000.101739	12.133466	-0.115790	4.817451
594.203254	8000.012252	12.138471	-0.115780	4.817425
594.257403	8000.065859	12.143475	-0.115790	4.817441
594.394427	8000.094304	12.148480	-0.115816	4.817448
594.107294	7999.989689	12.153485	-0.115762	4.817419
594.468181	8000.160873	12.158490	-0.115829	4.817468
594.658518	7999.972577	12.163495	-0.115865	4.817411
594.195378	8000.109268	12.168499	-0.115778	4.817454
594.243742	8000.094148	12.173504	-0.115787	4.817449
594.583991	7999.949277	12.178509	-0.115851	4.817405
594.249394	8000.037202	12.183514	-0.115788	4.817432
594.415994	8000.148458	12.188519	-0.115819	4.817464
595.042052	8000.187384	12.193523	-0.115936	4.817473
594.993760	8000.152866	12.198528	-0.115927	4.817463
595.073303	8000.331466	12.203533	-0.115942	4.817516
595.272719	8000.243626	12.208538	-0.115979	4.817489
595.515251	8000.307446	12.213543	-0.116024	4.817507
594.935983	8000.404381	12.218547	-0.115916	4.817538
595.139634	8000.274363	12.223552	-0.115954	4.817498
595.330114	8000.209623	12.228557	-0.115989	4.817478
595.048122	8000.238139	12.233562	-0.115937	4.817488
595.197703	8000.286839	12.238567	-0.115965	4.817502
595.106115	8000.346716	12.243571	-0.115948	4.817520
594.910249	8000.004799	12.248576	-0.115911	4.817420
594.530859	8000.165974	12.253581	-0.115840	4.817469
594.640471	8000.136985	12.258586	-0.115861	4.817460
594.989552	7999.998582	12.263591	-0.115925	4.817418
594.880103	8000.191251	12.268595	-0.115905	4.817475
594.843535	8000.130508	12.273600	-0.115898	4.817457
595.014803	8000.255565	12.278605	-0.115930	4.817493
595.054773	8000.258272	12.283610	-0.115938	4.817494
595.245674	8000.223107	12.288615	-0.115973	4.817483
595.080063	8000.234355	12.293619	-0.115942	4.817487
595.220578	8000.238565	12.298624	-0.115968	4.817487
595.446335	8000.274677	12.303629	-0.116010	4.817497
595.255618	8000.258092	12.308634	-0.115975	4.817493
595.531923	8000.358323	12.313639	-0.116026	4.817522
595.499448	8000.280742	12.318643	-0.116020	4.817499
595.343518	8000.370282	12.323648	-0.115991	4.817526
595.440040	8000.353770	12.328653	-0.116009	4.817521
595.494107	8000.251083	12.333658	-0.116019	4.817490
595.209180	8000.414729	12.338663	-0.115966	4.817540
594.961577	8000.213543	12.343667	-0.115920	4.817481
595.280651	8000.399951	12.348672	-0.115979	4.817535
595.286456	8000.373634	12.353677	-0.115980	4.817527
595.155857	8000.426591	12.358682	-0.115956	4.817543
595.137060	8000.168633	12.363687	-0.115952	4.817467
595.374647	8000.387616	12.368691	-0.115997	4.817531
595.440780	8000.355865	12.373696	-0.116009	4.817521
595.577916	8000.292438	12.378701	-0.116034	4.817502
595.413205	8000.360726	12.383706	-0.116004	4.817523
595.204535	8000.323808	12.388711	-0.115965	4.817513
594.900128	8000.229489	12.393715	-0.115908	4.817486
595.356040	8000.092683	12.398720	-0.115993	4.817444
595.382971	8000.318019	12.403725	-0.115998	4.817510
595.249959	8000.311802	12.408730	-0.115973	4.817509
595.379619	8000.273609	12.413735	-0.115997	4.817497
595.021383	8000.333722	12.418739	-0.115930	4.817517
595.197456	8000.193787	12.423744	-0.115963	4.817474
595.267729	8000.371194	12.428749	-0.115976	4.817527
595.321466	8000.228373	12.433754	-0.115986	4.817484
595.465166	8000.160820	12.438759	-0.116013	4.817463
595.179913	8000.162887	12.443763	-0.115960	4.817465
595.349518	8000.193934	12.448768	-0.115991	4.817474
595.189401	8000.297139	12.453773	-0.115961	4.817505
595.371593	8000.265012	12.458778	-0.115995	4.817495
595.152163	8000.203645	12.463783	-0.115954	4.817478
594.989220	8000.215989	12.468787	-0.115924	4.817482
595.340255	8000.163154	12.473792	-0.115989	4.817465
595.359268	8000.345075	12.478797	-0.115993	4.817518
595.403736	8000.155649	12.483802	-0.116001	4.817462
595.236231	8000.168981	12.488807	-0.115970	4.817467
595.008995	8000.122283	12.493811	-0.115927	4.817454
595.069377	8000.041868	12.498816	-0.115938	4.817430
594.695856	8000.157723	12.503821	-0.115869	4.817466
594.838582	8000.158798	12.508826	-0.115896	4.817466
594.885151	8000.162659	12.513831	-0.115904	4.817467
594.716598	8000.175976	12.518835	-0.115873	4.817471
594.844956	7999.985697	12.523840	-0.115896	4.817414
594.966715	8000.094172	12.528845	-0.115919	4.817446
595.279385	8000.268866	12.533850	-0.115977	4.817496
594.827124	7999.962188	12.538855	-0.115893	4.817408
595.110306	8000.118486	12.543859	-0.115946	4.817453
595.238992	8000.059157	12.548864	-0.115970	4.817434
595.384067	8000.197552	12.553869	-0.115997	4.817475
595.204359	8000.224430	12.558874	-0.115963	4.817483
595.338985	8000.114501	12.563879	-0.115988	4.817450
595.464079	8000.168114	12.568883	-0.116012	4.817466
595.404606	8000.064786	12.573888	-0.116000	4.817435
595.346020	8000.081859	12.578893	-0.115989	4.817441
595.579563	8000.153992	12.583898	-0.116033	4.817461
595.602463	8000.123706	12.588903	-0.116037	4.817452
595.025535	8000.165764	12.593907	-0.115930	4.817467
595.070743	8000.034434	12.598912	-0.115938	4.817428
595.012297	8000.161335	12.603917	-0.115927	4.817466
595.437067	8000.239496	12.608922	-0.116006	4.817487
595.149144	8000.031372	12.613927	-0.115952	4.817427
594.954864	8000.179476	12.618931	-0.115916	4.817471
594.957835	7999.959865	12.623936	-0.115917	4.817406
594.614582	7999.961067	12.628941	-0.115853	4.817408
594.572657	7999.963605	12.633946	-0.115845	4.817409
594.729130	7999.974389	12.638951	-0.115874	4.817412
594.650556	7999.983771	12.643955	-0.115859	4.817415
594.598423	8000.103374	12.648960	-0.115850	4.817450
594.046860	7999.874423	12.653965	-0.115747	4.817385
594.438201	7999.997484	12.658970	-0.115820	4.817420
594.700247	7999.920085	12.663975	-0.115868	4.817396
594.897125	8000.228214	12.668979	-0.115905	4.817486
595.074452	8000.268880	12.673984	-0.115938	4.817497
594.760503	8000.056145	12.678989	-0.115880	4.817436
594.846297	8000.155635	12.683994	-0.115896	4.817465
595.148424	7999.989073	12.688999	-0.115952	4.817414
595.081758	8000.234128	12.694003	-0.115939	4.817487
594.743223	8000.040034	12.699008	-0.115876	4.817431
595.162882	8000.081154	12.704013	-0.115954	4.817441
595.119488	8000.024533	12.709018	-0.115946	4.817425
594.883443	8000.009384	12.714023	-0.115902	4.817421
594.939887	8000.066194	12.719027	-0.115913	4.817438
594.940288	7999.966931	12.724032	-0.115913	4.817409
594.000356	7999.844114	12.729037	-0.115738	4.817376
594.567387	7999.936007	12.734042	-0.115843	4.817401
594.830716	7999.911427	12.739047	-0.115892	4.817393
595.121207	8000.150203	12.744051	-0.115946	4.817462
595.112974	7999.943097	12.749056	-0.115945	4.817401
595.181924	8000.154273	12.754061	-0.115958	4.817463
595.267912	8000.168228	12.759066	-0.115974	4.817467
595.443631	8000.263785	12.764071	-0.116006	4.817494
595.457147	8000.190061	12.769075	-0.116009	4.817472
595.608086	8000.150074	12.774080	-0.116037	4.817460
594.975267	8000.052957	12.779085	-0.115919	4.817434
595.190876	8000.129043	12.784090	-0.115959	4.817455
595.506552	8000.073567	12.789095	-0.116018	4.817438
595.450044	8000.275479	12.794099	-0.116007	4.817497
595.316642	7999.991519	12.799104	-0.115982	4.817414
595.176623	8000.116145	12.804109	-0.115956	4.817452
595.314788	8000.132993	12.809114	-0.115982	4.817456
595.462534	7999.987355	12.814119	-0.116009	4.817412
595.164439	8000.125458	12.819123	-0.115954	4.817454
595.360997	8000.135786	12.824128	-0.115990	4.817457
595.510420	8000.184484	12.829133	-0.116018	4.817470
595.748929	8000.245075	12.834138	-0.116063	4.817487
595.578586	8000.155928	12.839143	-0.116031	4.817462
595.317215	8000.280852	12.844147	-0.115982	4.817500
595.209947	8000.165193	12.849152	-0.115962	4.817466
595.532806	8000.063358	12.854157	-0.116022	4.817434
595.530858	8000.231237	12.859162	-0.116022	4.817484
595.691699	8000.266377	12.864167	-0.116052	4.817494
595.214589	8000.157857	12.869171	-0.115963	4.817464
594.985598	8000.118525	12.874176	-0.115920	4.817453
594.423779	8000.095338	12.879181	-0.115815	4.817449
594.363529	7999.884290	12.884186	-0.115804	4.817387
594.819659	8000.014656	12.889191	-0.115889	4.817423
595.246122	8000.222731	12.894195	-0.115968	4.817483
595.087990	8000.192906	12.899200	-0.115939	4.817475
595.406485	8000.230404	12.904205	-0.115998	4.817484
595.264574	8000.236726	12.909210	-0.115972	4.817487
595.023638	8000.137021	12.914215	-0.115927	4.817458
594.737880	8000.148585	12.919219	-0.115874	4.817463
595.349643	8000.214756	12.924224	-0.115987	4.817480
595.729004	8000.182410	12.929229	-0.116058	4.817469
595.631456	8000.268600	12.934234	-0.116040	4.817495
595.635984	8000.128210	12.939239	-0.116041	4.817453
595.513235	8000.243592	12.944243	-0.116018	4.817488
595.605149	8000.046428	12.949248	-0.116035	4.817429
595.182492	8000.099242	12.954253	-0.115956	4.817447
595.163018	7999.929984	12.959258	-0.115952	4.817397
595.254179	7999.977808	12.964263	-0.115969	4.817410
595.084596	8000.135785	12.969267	-0.115938	4.817458
595.559332	8000.144994	12.974272	-0.116026	4.817458
595.211753	8000.169362	12.979277	-0.115961	4.817467
595.070660	7999.971884	12.984282	-0.115935	4.817409
595.415340	8000.073133	12.989287	-0.115999	4.817438
595.059833	8000.236778	12.994291	-0.115933	4.817488
594.753904	7999.993540	12.999296	-0.115876	4.817417
594.999466	8000.029944	13.004301	-0.115922	4.817427
595.165647	7999.961672	13.009306	-0.115952	4.817406
594.850241	7999.970682	13.014311	-0.115894	4.817410
594.590176	7999.931944	13.019315	-0.115845	4.817400
594.814988	7999.923685	13.024320	-0.115887	4.817396
595.041929	7999.891169	13.029325	-0.115929	4.817386
595.321271	8000.111827	13.034330	-0.115981	4.817450
595.297374	7999.963623	13.039335	-0.115977	4.817406
594.454366	7999.888714	13.044339	-0.115820	4.817388
594.824519	7999.897411	13.049344	-0.115888	4.817389
595.028041	7999.969091	13.054349	-0.115926	4.817409
594.910711	7999.988454	13.059354	-0.115905	4.817415
594.696015	7999.861689	13.064359	-0.115864	4.817379
594.771955	7999.962085	13.069363	-0.115879	4.817408
594.850889	7999.910461	13.074368	-0.115893	4.817392
595.084928	7999.930853	13.079373	-0.115937	4.817397
594.366263	7999.898988	13.084378	-0.115803	4.817391
594.214818	7999.844979	13.089383	-0.115775	4.817376
594.427900	7999.969599	13.094387	-0.115814	4.817412
594.690018	7999.841513	13.099392	-0.115863	4.817373
594.832345	8000.121368	13.104397	-0.115890	4.817455
595.113613	7999.971391	13.109402	-0.115942	4.817409
595.283351	7999.949637	13.114407	-0.115973	4.817402
595.128174	8000.138454	13.119411	-0.115945	4.817458
594.854595	7999.843957	13.124416	-0.115893	4.817373
595.048625	7999.977799	13.129421	-0.115930	4.817411
594.753356	7999.877286	13.134426	-0.115875	4.817383
594.967843	7999.944905	13.139431	-0.115914	4.817402
594.838081	7999.968306	13.144435	-0.115890	4.817409
594.543494	7999.807612	13.149440	-0.115835	4.817363
594.361650	7999.950619	13.154445	-0.115802	4.817406
594.470296	7999.898384	13.159450	-0.115822	4.817390
594.935929	7999.813467	13.164455	-0.115908	4.817363
594.662269	7999.886462	13.169459	-0.115857	4.817386
595.088636	7999.942464	13.174464	-0.115937	4.817401
595.215472	7999.947526	13.179469	-0.115960	4.817402
595.180234	8000.000853	13.184474	-0.115954	4.817418
595.058912	7999.888154	13.189479	-0.115931	4.817385
595.487565	7999.934688	13.194483	-0.116011	4.817397
595.760559	8000.127797	13.199488	-0.116062	4.817453
595.527225	8000.146481	13.204493	-0.116018	4.817459
595.270088	7999.974724	13.209498	-0.115970	4.817409
595.176683	7999.895179	13.214503	-0.115953	4.817386
595.151270	8000.075375	13.219507	-0.115948	4.817440
595.050041	7999.940800	13.224512	-0.115929	4.817400
594.920662	7999.989551	13.229517	-0.115905	4.817415
594.678704	7999.882443	13.234522	-0.115860	4.817385
594.479445	7999.836166	13.239527	-0.115823	4.817372
594.479375	7999.901634	13.244531	-0.115823	4.817391
594.874237	7999.856844	13.249536	-0.115896	4.817376
594.649404	7999.991817	13.254541	-0.115854	4.817417
594.617683	7999.878347	13.259546	-0.115848	4.817384
595.081584	7999.779677	13.264551	-0.115935	4.817353
594.857026	8000.060384	13.269555	-0.115893	4.817437
595.134435	7999.815309	13.274560	-0.115944	4.817363
595.098293	8000.096722	13.279565	-0.115938	4.817446
595.245949	7999.946859	13.284570	-0.115965	4.817401
595.128455	8000.058093	13.289575	-0.115943	4.817435
595.165101	7999.947756	13.294579	-0.115950	4.817402
595.012402	7999.817693	13.299584	-0.115921	4.817364
594.995930	8000.078279	13.304589	-0.115919	4.817441
595.075918	7999.980206	13.309594	-0.115933	4.817412
595.467371	7999.951206	13.314599	-0.116006	4.817402
595.238161	7999.944608	13.319603	-0.115963	4.817401
594.982500	7999.979856	13.324608	-0.115916	4.817412
595.058156	7999.921847	13.329613	-0.115930	4.817395
595.259206	7999.966034	13.334618	-0.115967	4.817407
595.492518	7999.984303	13.339623	-0.116011	4.817411
595.480796	8000.100288	13.344627	-0.116008	4.817446
595.598451	7999.989049	13.349632	-0.116030	4.817412
595.743881	8000.115833	13.354637	-0.116057	4.817449
595.443828	8000.064877	13.359642	-0.116001	4.817435
595.809406	8000.018595	13.364647	-0.116069	4.817420
595.116342	7999.962820	13.369651	-0.115940	4.817407
595.407009	7999.852056	13.374656	-0.115994	4.817373
595.036209	7999.879247	13.379661	-0.115925	4.817382
595.069053	7999.852278	13.384666	-0.115931	4.817374
595.498028	7999.986466	13.389671	-0.116011	4.817412
595.470033	8000.095872	13.394675	-0.116006	4.817444
595.603175	7999.916222	13.399680	-0.116031	4.817391
595.907580	8000.071785	13.404685	-0.116087	4.817435
595.693111	8000.149889	13.409690	-0.116048	4.817459
596.012648	7999.979362	13.414695	-0.116107	4.817408
595.614610	8000.079010	13.419699	-0.116033	4.817439
595.451476	7999.996308	13.424704	-0.116002	4.817415
595.110582	7999.877159	13.429709	-0.115939	4.817381
595.451801	8000.008979	13.434714	-0.116002	4.817419
595.818577	8000.054591	13.439719	-0.116071	4.817431
595.701920	7999.971528	13.444723	-0.116049	4.817407
595.930182	8000.025628	13.449728	-0.116091	4.817422
595.612797	8000.046223	13.454733	-0.116032	4.817429
595.722646	8000.039415	13.459738	-0.116053	4.817427
595.646805	7999.911554	13.464743	-0.116038	4.817389
594.918786	8000.007324	13.469747	-0.115903	4.817421
594.800551	7999.866160	13.474752	-0.115881	4.817379
595.411064	7999.930196	13.479757	-0.115994	4.817396
595.277801	8000.070764	13.484762	-0.115970	4.817438
595.420604	7999.870139	13.489767	-0.115996	4.817378
595.261762	8000.043061	13.494771	-0.115966	4.817430
595.389376	7999.945699	13.499776	-0.115990	4.817400
595.315591	8000.009010	13.504781	-0.115976	4.817419
595.601795	8000.110442	13.509786	-0.116030	4.817448
595.655001	7999.894748	13.514791	-0.116039	4.817384
595.391475	7999.961558	13.519795	-0.115990	4.817405
595.577730	8000.070999	13.524800	-0.116025	4.817437
595.694449	8000.122376	13.529805	-0.116047	4.817451
595.810174	8000.128328	13.534810	-0.116068	4.817453
595.498928	7999.921968	13.539815	-0.116010	4.817393
595.000609	7999.959923	13.544819	-0.115917	4.817406
595.376442	7999.843041	13.549824	-0.115987	4.817370
595.413226	8000.052680	13.554829	-0.115994	4.817432
595.106884	7999.972063	13.559834	-0.115937	4.817409
595.620259	7999.959671	13.564839	-0.116033	4.817404
595.455173	8000.000496	13.569843	-0.116002	4.817416
595.635537	7999.907092	13.574848	-0.116035	4.817388
595.491734	8000.034830	13.579853	-0.116009	4.817426
595.363378	8000.030795	13.584858	-0.115985	4.817426
595.028475	7999.891671	13.589863	-0.115922	4.817386
594.963210	7999.930820	13.594867	-0.115910	4.817398
595.519905	7999.937028	13.599872	-0.116014	4.817397
596.037361	8000.150691	13.604877	-0.116110	4.817458
596.101798	8000.363920	13.609882	-0.116122	4.817521
596.239762	8000.153713	13.614887	-0.116148	4.817458
596.379956	8000.354348	13.619891	-0.116174	4.817517
596.411136	8000.263989	13.624896	-0.116180	4.817490
595.944547	8000.263341	13.629901	-0.116093	4.817492
596.036187	8000.219298	13.634906	-0.116110	4.817478
595.626892	7999.972395	13.639911	-0.116033	4.817407
595.613100	8000.080957	13.644915	-0.116031	4.817439
595.515376	8000.007682	13.649920	-0.116012	4.817418
595.608658	8000.093557	13.654925	-0.116030	4.817443
595.647318	8000.171223	13.659930	-0.116037	4.817466
595.837858	7999.939629	13.664935	-0.116072	4.817397
595.474086	8000.114767	13.669939	-0.116005	4.817450
595.212611	7999.835233	13.674944	-0.115956	4.817369
595.514479	8000.161831	13.679949	-0.116012	4.817464
595.709364	8000.081315	13.684954	-0.116048	4.817439
595.647502	8000.061378	13.689959	-0.116037	4.817433
595.612347	8000.046065	13.694963	-0.116030	4.817429
595.800044	8000.087942	13.699968	-0.116065	4.817441
595.547819	7999.964835	13.704973	-0.116018	4.817405
595.263963	7999.986989	13.709978	-0.115965	4.817413
595.498832	8000.009506	13.714983	-0.116009	4.817419
595.622230	8000.024020	13.719987	-0.116032	4.817423
595.585247	8000.066761	13.724992	-0.116025	4.817435
595.474664	7999.984846	13.729997	-0.116004	4.817412
595.998552	8000.157421	13.735002	-0.116102	4.817460
595.761968	7999.966959	13.740007	-0.116058	4.817405
595.587472	8000.151265	13.745011	-0.116025	4.817460
595.459802	7999.831488	13.750016	-0.116001	4.817366
595.448470	7999.895733	13.755021	-0.115999	4.817385
595.833696	8000.014485	13.760026	-0.116071	4.817419
595.345997	7999.862514	13.765031	-0.115980	4.817376
595.717329	7999.938816	13.770035	-0.116049	4.817397
595.646198	7999.947254	13.775040	-0.116036	4.817400
595.263010	7999.951026	13.780045	-0.115964	4.817403
595.612214	7999.972084	13.785050	-0.116029	4.817407
595.432865	7999.911318	13.790055	-0.115996	4.817390
595.779232	8000.024209	13.795059	-0.116060	4.817422
595.841343	7999.929035	13.800064	-0.116072	4.817394
595.140988	7999.860480	13.805069	-0.115941	4.817376
594.658973	7999.926137	13.810074	-0.115852	4.817398
594.586402	7999.866970	13.815079	-0.115838	4.817381
595.171057	7999.893657	13.820083	-0.115947	4.817386
594.782763	7999.874122	13.825088	-0.115875	4.817382
595.167400	7999.981245	13.830093	-0.115946	4.817412
595.207991	7999.956504	13.835098	-0.115954	4.817404
595.641644	7999.921800	13.840103	-0.116034	4.817392
595.408589	8000.070380	13.845107	-0.115991	4.817437
595.285553	7999.863669	13.850112	-0.115968	4.817377
595.322187	7999.906454	13.855117	-0.115975	4.817389
595.677983	8000.035326	13.860122	-0.116041	4.817426
595.173399	7999.902111	13.865127	-0.115947	4.817389
594.911192	7999.906637	13.870131	-0.115898	4.817391
594.571945	7999.870940	13.875136	-0.115835	4.817382
594.540633	7999.850405	13.880141	-0.115829	4.817376
594.294493	7999.964995	13.885146	-0.115783	4.817411
594.813876	7999.897778	13.890151	-0.115880	4.817389
595.137701	7999.804406	13.895155	-0.115940	4.817360
595.510610	7999.924027	13.900160	-0.116010	4.817394
595.382057	8000.021368	13.905165	-0.115986	4.817423
595.659944	8000.013904	13.910170	-0.116037	4.817419
595.575856	8000.071781	13.915175	-0.116022	4.817437
595.767599	8000.050357	13.920179	-0.116057	4.817430
595.638242	8000.092773	13.925184	-0.116033	4.817443
595.884857	7999.978182	13.930189	-0.116079	4.817408
595.530739	7999.969715	13.935194	-0.116013	4.817407
595.602406	7999.943327	13.940199	-0.116026	4.817399
595.334187	7999.988946	13.945203	-0.115976	4.817414
595.269181	7999.864417	13.950208	-0.115964	4.817377
595.480308	7999.888690	13.955213	-0.116003	4.817383
595.051620	7999.898119	13.960218	-0.115924	4.817388
595.055083	7999.822135	13.965223	-0.115924	4.817365
595.307698	8000.059288	13.970227	-0.115971	4.817434
595.507737	7999.928161	13.975232	-0.116008	4.817395
595.616900	8000.162117	13.980237	-0.116029	4.817463
595.498182	7999.934348	13.985242	-0.116007	4.817397
595.440867	7999.888079	13.990247	-0.115996	4.817383
595.140314	7999.964896	13.995251	-0.115940	4.817407
595.566813	7999.968101	14.000256	-0.116019	4.817406
595.872601	7999.983231	14.005261	-0.116076	4.817409
595.273607	7999.847549	14.010266	-0.115965	4.817372
595.116924	7999.912789	14.015271	-0.115935	4.817392
595.123084	7999.889645	14.020275	-0.115936	4.817385
595.186156	7999.864185	14.025280	-0.115948	4.817377
595.250981	7999.891551	14.030285	-0.115960	4.817385
594.906615	7999.851552	14.035290	-0.115896	4.817375
595.162088	7999.930344	14.040295	-0.115944	4.817397
595.479490	7999.965711	14.045299	-0.116003	4.817406
595.137371	7999.882448	14.050304	-0.115939	4.817383
595.254375	7999.957059	14.055309	-0.115961	4.817404
595.211126	8000.053563	14.060314	-0.115953	4.817433
594.913762	7999.803064	14.065319	-0.115897	4.817360
594.939129	7999.876304	14.070323	-0.115902	4.817382
595.046773	7999.855734	14.075328	-0.115922	4.817375
595.419929	7999.889821	14.080333	-0.115991	4.817384
595.045846	7999.971875	14.085338	-0.115922	4.817410
595.382662	7999.909322	14.090343	-0.115984	4.817390
594.507858	7999.831827	14.095347	-0.115821	4.817371
594.871858	7999.892176	14.100352	-0.115889	4.817387
594.847997	7999.958345	14.105357	-0.115885	4.817407
594.878242	7999.820457	14.110362	-0.115890	4.817366
595.161059	7999.901769	14.115367	-0.115943	4.817389
594.997398	7999.924664	14.120371	-0.115912	4.817396
594.484017	7999.909596	14.125376	-0.115817	4.817394
594.681126	7999.867130	14.130381	-0.115853	4.817380
595.053925	7999.958236	14.135386	-0.115923	4.817406
594.820856	7999.856540	14.140391	-0.115879	4.817377
595.040553	7999.947470	14.145395	-0.115920	4.817403
594.620268	7999.831360	14.150400	-0.115842	4.817370
594.548499	7999.872525	14.155405	-0.115828	4.817383
594.735325	7999.938674	14.160410	-0.115863	4.817401
594.882756	7999.868010	14.165415	-0.115891	4.817380
594.756015	7999.836544	14.170419	-0.115867	4.817371
595.124154	7999.986717	14.175424	-0.115935	4.817414
594.931226	7999.808532	14.180429	-0.115899	4.817362
594.870418	7999.906885	14.185434	-0.115888	4.817391
594.971828	7999.826029	14.190439	-0.115907	4.817367
594.657150	7999.866731	14.195443	-0.115848	4.817380
594.825775	7999.908320	14.200448	-0.115880	4.817392
594.680355	7999.944160	14.205453	-0.115853	4.817403
594.616162	7999.841821	14.210458	-0.115841	4.817373
594.943825	7999.849883	14.215463	-0.115902	4.817374
595.311787	7999.990550	14.220467	-0.115970	4.817414
595.225951	7999.874157	14.225472	-0.115954	4.817380
594.771937	7999.873704	14.230477	-0.115869	4.817382
594.789724	7999.911983	14.235482	-0.115873	4.817393
594.988372	7999.804069	14.240487	-0.115910	4.817360
595.410931	7999.989904	14.245491	-0.115988	4.817414
595.081024	7999.920552	14.250496	-0.115927	4.817394
594.935207	7999.845505	14.255501	-0.115900	4.817373
595.422292	7999.859118	14.260506	-0.115990	4.817375
595.608855	7999.970675	14.265511	-0.116025	4.817407
595.095084	7999.932366	14.270515	-0.115929	4.817398
595.617484	7999.961293	14.275520	-0.116027	4.817404
595.930202	7999.957518	14.280525	-0.116085	4.817402
595.595069	7999.958840	14.285530	-0.116022	4.817404
595.574661	7999.981764	14.290535	-0.116018	4.817410
595.428688	7999.951065	14.295539	-0.115991	4.817402
595.581150	7999.999807	14.300544	-0.116020	4.817416
595.451588	7999.876424	14.305549	-0.115995	4.817380
595.135775	7999.897044	14.310554	-0.115937	4.817387
595.338510	7999.893736	14.315559	-0.115974	4.817385
595.023327	7999.839389	14.320563	-0.115915	4.817371
595.156417	7999.868831	14.325568	-0.115940	4.817379
595.406657	7999.886297	14.330573	-0.115987	4.817383
595.437443	7999.968067	14.335578	-0.115993	4.817407
595.294579	7999.812806	14.340583	-0.115966	4.817362
595.568486	8000.014374	14.345587	-0.116017	4.817420
595.390526	7999.811066	14.350592	-0.115984	4.817361
595.147363	7999.958438	14.355597	-0.115938	4.817405
594.922059	7999.868474	14.360602	-0.115896	4.817380
595.277299	7999.886453	14.365607	-0.115962	4.817384
595.391897	7999.795233	14.370611	-0.115984	4.817356
595.360087	7999.932037	14.375616	-0.115978	4.817397
595.599876	7999.911330	14.380621	-0.116022	4.817389
595.127225	7999.846181	14.385626	-0.115934	4.817372
595.394553	7999.951551	14.390631	-0.115984	4.817402
595.514862	7999.875201	14.395635	-0.116006	4.817379
595.390165	7999.858549	14.400640	-0.115983	4.817375
595.407539	7999.940120	14.405645	-0.115986	4.817399
595.288810	7999.895045	14.410650	-0.115964	4.817386
595.908218	7999.857837	14.415655	-0.116080	4.817372
595.689475	7999.944326	14.420659	-0.116039	4.817399
596.003511	7999.938458	14.425664	-0.116097	4.817396
596.303112	7999.939768	14.430669	-0.116153	4.817395
596.229994	7999.947119	14.435674	-0.116139	4.817397
595.673093	7999.926115	14.440679	-0.116036	4.817394
595.115040	7999.934665	14.445683	-0.115932	4.817399
595.370226	7999.856108	14.450688	-0.115979	4.817374
595.389228	7999.951430	14.455693	-0.115983	4.817402
595.296823	7999.885629	14.460698	-0.115965	4.817383
595.238630	7999.880532	14.465703	-0.115954	4.817382
594.954363	7999.855159	14.470707	-0.115901	4.817376
594.975820	7999.848085	14.475712	-0.115905	4.817374
595.274871	7999.946537	14.480717	-0.115961	4.817401
595.131481	7999.836677	14.485722	-0.115934	4.817369
595.060542	7999.610686	14.490727	-0.115921	4.817303

595.238694	7996.331639	14.495731	-0.115952	4.816333
595.223219	7990.768384	14.500736	-0.115945	4.814687
595.274291	7984.081245	14.505741	-0.115950	4.812709
595.019655	7976.757619	14.510746	-0.115898	4.810542
595.239624	7969.165870	14.515751	-0.115934	4.808293
594.910642	7961.331814	14.520755	-0.115868	4.805973
595.087767	7953.375991	14.525760	-0.115896	4.803614
595.199506	7945.553632	14.530765	-0.115911	4.801294
594.555762	7937.514482	14.535770	-0.115786	4.798911
594.758367	7929.584359	14.540775	-0.115819	4.796556
595.006345	7921.460034	14.545779	-0.115859	4.794142
595.142750	7913.551507	14.550784	-0.115880	4.791792
594.895117	7905.529622	14.555789	-0.115828	4.789408
594.408204	7897.578109	14.560794	-0.115732	4.787045
594.380602	7889.566081	14.565799	-0.115722	4.784660
594.143044	7881.584884	14.570803	-0.115673	4.782285
594.785678	7873.489332	14.575808	-0.115787	4.779871
594.442356	7865.561002	14.580813	-0.115718	4.777509
594.567920	7857.441151	14.585818	-0.115736	4.775087
594.491233	7849.545931	14.590823	-0.115716	4.772732
594.583824	7841.475626	14.595827	-0.115728	4.770323
594.899876	7833.468246	14.600832	-0.115782	4.767930
594.573249	7825.515342	14.605837	-0.115716	4.765555
594.831638	7817.455752	14.610842	-0.115759	4.763145
594.721450	7809.536183	14.615847	-0.115733	4.760777
594.790560	7801.527505	14.620851	-0.115741	4.758380
594.519797	7793.512171	14.625856	-0.115685	4.755981
594.664765	7785.492539	14.630861	-0.115707	4.753578
594.823458	7777.458300	14.635866	-0.115731	4.751170
594.612183	7769.482915	14.640871	-0.115686	4.748779
594.532649	7761.443136	14.645875	-0.115666	4.746367
594.873488	7753.419568	14.650880	-0.115724	4.743958
594.414583	7745.549882	14.655885	-0.115634	4.741596
594.361707	7737.438470	14.660890	-0.115619	4.739159
594.250566	7729.521812	14.665895	-0.115593	4.736779
594.263155	7721.419251	14.670899	-0.115590	4.734342
594.420107	7713.448559	14.675904	-0.115614	4.731943
594.103035	7705.460539	14.680909	-0.115549	4.729539
594.251619	7697.455383	14.685914	-0.115572	4.727127
594.506038	7689.377376	14.690919	-0.115614	4.724692
593.763113	7681.501200	14.695923	-0.115470	4.722319
593.488773	7673.489796	14.700928	-0.115414	4.719902
593.779839	7665.510248	14.705933	-0.115463	4.717493
593.647842	7657.429555	14.710938	-0.115433	4.715053
593.572120	7649.468124	14.715943	-0.115414	4.712648
593.494456	7641.447806	14.720947	-0.115394	4.710223
593.143538	7633.428974	14.725952	-0.115323	4.707798
593.445652	7625.376982	14.730957	-0.115374	4.705361
593.638466	7617.369668	14.735962	-0.115405	4.702936
593.410859	7609.479516	14.740967	-0.115358	4.700546
593.021488	7601.474199	14.745971	-0.115280	4.698120
592.998969	7593.477094	14.750976	-0.115270	4.695695
593.580295	7585.367754	14.755981	-0.115373	4.693234
593.435451	7577.379347	14.760986	-0.115341	4.690809
593.259466	7569.441237	14.765991	-0.115303	4.688398
593.122329	7561.406800	14.770995	-0.115272	4.685957
593.290527	7553.336802	14.776000	-0.115298	4.683503
593.183162	7545.463816	14.781005	-0.115273	4.681108
593.267725	7537.366939	14.786010	-0.115284	4.678643
593.159199	7529.466314	14.791015	-0.115258	4.676237
593.228851	7521.348101	14.796019	-0.115266	4.673764
592.764508	7513.430104	14.801024	-0.115174	4.671351
592.659656	7505.378268	14.806029	-0.115149	4.668895
592.717441	7497.372073	14.811034	-0.115155	4.666452
593.078002	7489.312560	14.816039	-0.115217	4.663990
592.921079	7481.407168	14.821043	-0.115182	4.661576
592.579546	7473.371770	14.826048	-0.115113	4.659120
592.244358	7465.484671	14.831053	-0.115046	4.656708
592.385296	7457.358833	14.836058	-0.115067	4.654222
592.293371	7449.445934	14.841063	-0.115044	4.651799
592.278791	7441.366112	14.846067	-0.115036	4.649325
592.293215	7433.368044	14.851072	-0.115034	4.646873
592.150094	7425.351650	14.856077	-0.115002	4.644416
592.479977	7417.389790	14.861082	-0.115058	4.641973
592.427595	7409.376863	14.866087	-0.115043	4.639513
592.523965	7401.424171	14.871091	-0.115056	4.637071
591.867624	7393.406411	14.876096	-0.114928	4.634607
592.097031	7385.408418	14.881101	-0.114966	4.632149
592.347721	7377.302971	14.886106	-0.115007	4.629655
592.383409	7369.367189	14.891111	-0.115009	4.627213
592.281179	7361.359648	14.896115	-0.114984	4.624747
592.073993	7353.428434	14.901120	-0.114940	4.622304
592.388795	7345.344063	14.906125	-0.114994	4.619812
591.871070	7337.393420	14.911130	-0.114892	4.617359
591.916492	7329.356434	14.916135	-0.114895	4.614879
591.559659	7321.455795	14.921139	-0.114824	4.612440
591.321211	7313.384489	14.926144	-0.114774	4.609946
591.441510	7305.391682	14.931149	-0.114791	4.607476
591.479332	7297.310449	14.936154	-0.114793	4.604977
591.395757	7289.377114	14.941159	-0.114772	4.602522
590.904758	7281.380523	14.946163	-0.114675	4.600046
590.883001	7273.405302	14.951168	-0.114666	4.597575
591.035389	7265.361370	14.956173	-0.114689	4.595082
590.515983	7257.336922	14.961178	-0.114587	4.592593
590.512486	7249.309299	14.966183	-0.114581	4.590103
590.288844	7241.334065	14.971187	-0.114534	4.587627
590.534925	7233.242927	14.976192	-0.114575	4.585114
590.419561	7225.335304	14.981197	-0.114548	4.582656
590.567338	7217.276322	14.986202	-0.114571	4.580150
590.225160	7209.380297	14.991207	-0.114502	4.577693
590.349307	7201.291048	14.996211	-0.114519	4.575175
590.214195	7193.336695	15.001216	-0.114489	4.572698
590.057862	7185.352763	15.006221	-0.114455	4.570210
589.769628	7177.313855	15.011226	-0.114396	4.567703
589.780908	7169.285913	15.016231	-0.114393	4.565198
589.649371	7161.328153	15.021235	-0.114363	4.562714
589.866159	7153.282880	15.026240	-0.114398	4.560202
589.633841	7145.346462	15.031245	-0.114350	4.557721
589.105373	7137.321414	15.036250	-0.114246	4.555211
589.673072	7129.258268	15.041255	-0.114346	4.552690
589.936275	7121.170416	15.046259	-0.114390	4.550159
589.676089	7113.231947	15.051264	-0.114336	4.547672
589.553600	7105.323887	15.056269	-0.114308	4.545194
589.374561	7097.329999	15.061274	-0.114270	4.542687
589.415838	7089.234549	15.066279	-0.114272	4.540148
589.416591	7081.280152	15.071283	-0.114267	4.537651
589.818109	7073.195915	15.076288	-0.114336	4.535113
589.662958	7065.278316	15.081293	-0.114302	4.532625
589.218222	7057.222500	15.086298	-0.114214	4.530091
589.139879	7049.291414	15.091303	-0.114194	4.527596
588.545991	7041.289720	15.096307	-0.114079	4.525076
588.725742	7033.272231	15.101312	-0.114107	4.522552
588.745306	7025.242729	15.106317	-0.114105	4.520021
588.400475	7017.281370	15.111322	-0.114036	4.517510
588.463845	7009.281275	15.116327	-0.114042	4.514987
588.391085	7001.296796	15.121331	-0.114024	4.512467
588.521824	6993.150820	15.126336	-0.114043	4.509894
588.883171	6985.151413	15.131341	-0.114105	4.507368
588.821946	6977.134882	15.136346	-0.114088	4.504833
589.231029	6969.224697	15.141351	-0.114159	4.502332
588.838513	6961.219530	15.146355	-0.114081	4.499797
588.708128	6953.246838	15.151360	-0.114051	4.497271
588.912927	6945.153950	15.156365	-0.114084	4.494708
589.003579	6937.158398	15.161370	-0.114095	4.492173
589.322524	6929.102821	15.166375	-0.114150	4.489618
589.540661	6921.136427	15.171379	-0.114185	4.487091
589.527406	6913.112237	15.176384	-0.114177	4.484542
589.647873	6905.251158	15.181389	-0.114194	4.482045
589.465913	6897.148673	15.186394	-0.114155	4.479468
589.666976	6889.224869	15.191399	-0.114188	4.476948
589.324139	6881.187589	15.196403	-0.114118	4.474388
588.560966	6873.258275	15.201408	-0.113971	4.471859
588.800124	6865.183981	15.206413	-0.114010	4.469287
588.205411	6857.208146	15.211418	-0.113894	4.466741
588.531364	6849.111635	15.216423	-0.113950	4.464160
588.571711	6841.162292	15.221427	-0.113952	4.461622
588.661872	6833.097588	15.226432	-0.113963	4.459046
588.615920	6825.193663	15.231437	-0.113950	4.456520
588.640264	6817.115645	15.236442	-0.113949	4.453937
588.598239	6809.182727	15.241447	-0.113936	4.451398
588.330101	6801.165930	15.246451	-0.113881	4.448830
587.786569	6793.223116	15.251456	-0.113774	4.446284
587.974864	6785.144900	15.256461	-0.113804	4.443695
587.575851	6777.214300	15.261466	-0.113725	4.441150
587.992501	6769.177969	15.266471	-0.113797	4.438573
587.168786	6761.210643	15.271475	-0.113638	4.436011
587.427361	6753.097571	15.276480	-0.113681	4.433405
587.648394	6745.112089	15.281485	-0.113717	4.430839
587.614552	6737.056571	15.286490	-0.113705	4.428248
587.582085	6729.087228	15.291495	-0.113694	4.425683
587.590313	6721.122839	15.296499	-0.113690	4.423118
587.437065	6713.140527	15.301504	-0.113657	4.420545
587.874837	6705.117346	15.306509	-0.113733	4.417961
587.679100	6697.118960	15.311514	-0.113691	4.415380
587.307964	6689.202758	15.316519	-0.113617	4.412823
587.434594	6681.077916	15.321523	-0.113635	4.410199
587.365480	6673.084874	15.326528	-0.113617	4.407616
587.231454	6665.089968	15.331533	-0.113587	4.405030
587.013315	6657.099377	15.336538	-0.113541	4.402443
587.223266	6649.091459	15.341543	-0.113575	4.399852
586.558589	6641.224436	15.346547	-0.113446	4.397300
586.726964	6633.088962	15.351552	-0.113472	4.394664
586.792838	6625.121878	15.356557	-0.113479	4.392080
586.585993	6617.093381	15.361562	-0.113435	4.389474
586.329149	6609.158159	15.366567	-0.113382	4.386896
586.394803	6601.059217	15.371571	-0.113389	4.384265
586.716263	6593.093644	15.376576	-0.113444	4.381677
586.600732	6585.053838	15.381581	-0.113417	4.379061
586.442770	6577.085889	15.386586	-0.113382	4.376467
587.072104	6569.017996	15.391591	-0.113494	4.373843
586.770943	6561.124664	15.396595	-0.113433	4.371269
587.029736	6553.009413	15.401600	-0.113476	4.368625
586.670362	6545.071359	15.406605	-0.113404	4.366033
586.643646	6537.060566	15.411610	-0.113393	4.363417
587.376406	6529.054084	15.416615	-0.113525	4.360807
587.000911	6521.125990	15.421619	-0.113449	4.358213
586.435759	6513.192477	15.426624	-0.113339	4.355615
586.681610	6505.152167	15.431629	-0.113379	4.352986
586.768209	6497.101950	15.436634	-0.113390	4.350350
586.300458	6489.124860	15.441639	-0.113298	4.347733
586.166650	6481.127343	15.446643	-0.113268	4.345111
586.156996	6473.182392	15.451648	-0.113261	4.342504
585.759689	6465.198591	15.456653	-0.113182	4.339881
585.709163	6457.224319	15.461658	-0.113167	4.337262
585.217661	6449.236431	15.466663	-0.113070	4.334633
585.274150	6441.181228	15.471667	-0.113075	4.331985
585.363426	6433.099824	15.476672	-0.113087	4.329326
585.518546	6425.188663	15.481677	-0.113110	4.326723
585.768086	6417.037453	15.486682	-0.113151	4.324039
586.125434	6409.102633	15.491687	-0.113213	4.321427
586.046566	6401.127079	15.496691	-0.113193	4.318795
585.548265	6393.240299	15.501696	-0.113095	4.316188
585.226511	6385.227559	15.506701	-0.113030	4.313540
585.177060	6377.170706	15.511706	-0.113015	4.310877
585.342393	6369.140930	15.516711	-0.113041	4.308223
585.358932	6361.077295	15.521715	-0.113039	4.305556
585.207956	6353.089796	15.526720	-0.113005	4.302910
585.418543	6345.109446	15.531725	-0.113039	4.300268
585.058336	6337.124921	15.536730	-0.112967	4.297618
585.598693	6329.029202	15.541735	-0.113062	4.294938
585.453715	6321.094290	15.546739	-0.113030	4.292303
585.519654	6313.003748	15.551744	-0.113037	4.289617
585.454586	6305.097334	15.556749	-0.113020	4.286989
585.305201	6297.044088	15.561754	-0.112987	4.284310
585.183999	6289.187504	15.566759	-0.112959	4.281695
585.097920	6281.116396	15.571763	-0.112937	4.279008
585.052542	6273.168289	15.576768	-0.112924	4.276359
585.362453	6265.059096	15.581773	-0.112976	4.273659
584.992503	6257.148528	15.586778	-0.112902	4.271017
584.856565	6249.085993	15.591783	-0.112871	4.268325
584.679506	6241.110123	15.596787	-0.112833	4.265660
584.578140	6233.080227	15.601792	-0.112809	4.262976
584.826044	6225.067058	15.606797	-0.112850	4.260299
584.789366	6217.103291	15.611802	-0.112838	4.257634
584.587954	6209.109156	15.616807	-0.112795	4.254955
584.690967	6201.085299	15.621811	-0.112809	4.252268
584.834684	6193.033647	15.626816	-0.112831	4.249571
585.047769	6185.088312	15.631821	-0.112865	4.246907
584.786316	6177.017686	15.636826	-0.112811	4.244196
584.546155	6169.151491	15.641831	-0.112761	4.241552
584.737256	6161.079674	15.646835	-0.112791	4.238841
584.831411	6153.071537	15.651840	-0.112804	4.236149
584.267255	6145.182899	15.656845	-0.112694	4.233488
584.174137	6137.086818	15.661850	-0.112671	4.230761
584.401055	6129.081643	15.666855	-0.112708	4.228066
584.146522	6121.099977	15.671859	-0.112655	4.225373
583.997311	6113.101756	15.676864	-0.112622	4.222673
583.934871	6105.103246	15.681869	-0.112605	4.219972
584.234483	6097.077308	15.686874	-0.112656	4.217264
584.306148	6089.042353	15.691879	-0.112664	4.214549
583.970600	6081.108504	15.696883	-0.112596	4.211862
583.813698	6073.077343	15.701888	-0.112562	4.209142
583.429847	6065.156408	15.706893	-0.112485	4.206455
583.174981	6057.090108	15.711898	-0.112432	4.203719
583.227161	6049.158172	15.716903	-0.112437	4.201029
583.430078	6041.093937	15.721907	-0.112469	4.198295
583.133771	6033.086209	15.726912	-0.112409	4.195573
583.265516	6025.056801	15.731917	-0.112428	4.192846
583.251291	6017.025491	15.736922	-0.112420	4.190115
583.249317	6009.011862	15.741927	-0.112415	4.187389
582.940439	6001.033036	15.746931	-0.112352	4.184669
582.582910	5993.121643	15.751936	-0.112280	4.181969
582.660698	5985.058791	15.756941	-0.112289	4.179222
582.901082	5977.038656	15.761946	-0.112329	4.176489
583.347352	5968.982764	15.766951	-0.112407	4.173744
583.170873	5961.065937	15.771955	-0.112368	4.171038
583.028853	5953.004286	15.776960	-0.112337	4.168281
583.000832	5945.037124	15.781965	-0.112326	4.165556
582.877776	5937.066684	15.786970	-0.112298	4.162827
582.668499	5929.119162	15.791975	-0.112254	4.160102
582.430976	5921.097800	15.796979	-0.112204	4.157351
582.819202	5912.993940	15.801984	-0.112271	4.154576
582.968710	5905.114027	15.806989	-0.112294	4.151874
582.591791	5897.053717	15.811994	-0.112219	4.149102
583.054221	5889.066540	15.816999	-0.112299	4.146363
582.842502	5881.038295	15.822003	-0.112255	4.143600
582.801413	5873.077264	15.827008	-0.112242	4.140861
583.000847	5865.080008	15.832013	-0.112274	4.138110
582.648516	5857.075869	15.837018	-0.112203	4.135348
582.551551	5849.075847	15.842023	-0.112180	4.132589
582.413853	5841.051985	15.847027	-0.112149	4.129819
582.252483	5833.069723	15.852032	-0.112113	4.127061
582.322228	5825.089529	15.857037	-0.112121	4.124305
582.355089	5817.123276	15.862042	-0.112122	4.121552
582.666955	5809.024438	15.867047	-0.112175	4.118755
582.092988	5801.154421	15.872051	-0.112063	4.116023
582.102306	5793.103320	15.877056	-0.112059	4.113235
582.011421	5785.132712	15.882061	-0.112037	4.110471
582.306638	5777.075040	15.887066	-0.112087	4.107680
582.323605	5769.039050	15.892071	-0.112085	4.104891
581.751860	5761.162948	15.897075	-0.111973	4.102148
581.837528	5753.079508	15.902080	-0.111984	4.099339
581.413455	5745.168164	15.907085	-0.111899	4.096582
581.609276	5737.065328	15.912090	-0.111931	4.093765
581.888592	5729.059626	15.917095	-0.111977	4.090981
581.846855	5721.074038	15.922099	-0.111964	4.088197
581.623831	5713.042216	15.927104	-0.111918	4.085393
581.431387	5705.150693	15.932109	-0.111877	4.082636
581.693377	5697.050230	15.937114	-0.111920	4.079811
581.750094	5689.109306	15.942119	-0.111925	4.077037
581.394817	5681.093552	15.947123	-0.111854	4.074229
581.526092	5673.033808	15.952128	-0.111873	4.071410
581.367590	5665.100439	15.957133	-0.111838	4.068630
581.016677	5657.110287	15.962138	-0.111768	4.065824
580.892024	5649.161648	15.967143	-0.111739	4.063035
581.311916	5641.067380	15.972147	-0.111812	4.060201
581.001563	5633.105669	15.977152	-0.111749	4.057401
581.016559	5625.109034	15.982157	-0.111747	4.054591
581.418596	5617.056051	15.987162	-0.111816	4.051765
580.531913	5609.129773	15.992167	-0.111646	4.048962
580.451828	5601.142488	15.997171	-0.111626	4.046149
580.633714	5593.068798	16.002176	-0.111654	4.043306
580.758526	5585.104106	16.007181	-0.111672	4.040500
580.764947	5577.072276	16.012186	-0.111668	4.037665
580.587884	5569.097493	16.017191	-0.111630	4.034847
580.735250	5561.006238	16.022195	-0.111652	4.031990
581.048945	5552.923848	16.027200	-0.111705	4.029136
580.867578	5545.071157	16.032205	-0.111666	4.026355
580.939012	5537.012564	16.037210	-0.111674	4.023502
580.789147	5529.141379	16.042215	-0.111641	4.020711
580.436752	5521.140570	16.047219	-0.111571	4.017868
580.785838	5513.036281	16.052224	-0.111630	4.014997
580.899798	5505.058240	16.057229	-0.111646	4.012166
580.843045	5497.006680	16.062234	-0.111630	4.009304
580.507210	5489.109782	16.067239	-0.111563	4.006490
581.007946	5481.031673	16.072243	-0.111651	4.003623
580.597757	5473.135541	16.077248	-0.111569	4.000804
581.004137	5465.084463	16.082253	-0.111639	3.997942
580.572606	5457.148244	16.087258	-0.111554	3.995104
580.716985	5449.161906	16.092263	-0.111575	3.992256
580.306700	5441.128768	16.097267	-0.111494	3.989380
580.497142	5433.110659	16.102272	-0.111524	3.986518
580.780529	5425.109516	16.107277	-0.111571	3.983661
580.680849	5417.121853	16.112282	-0.111548	3.980800
580.689249	5409.138278	16.117287	-0.111544	3.977941
580.560057	5401.139218	16.122291	-0.111515	3.975071
580.144293	5393.189447	16.127296	-0.111432	3.972212
580.158664	5385.146433	16.132301	-0.111429	3.969325
580.089616	5377.164600	16.137306	-0.111411	3.966457
580.273041	5369.115440	16.142311	-0.111440	3.963567
580.326066	5361.121870	16.147315	-0.111445	3.960692
580.109172	5353.164750	16.152320	-0.111399	3.957823
580.219195	5345.173907	16.157325	-0.111414	3.954946
580.063857	5337.144911	16.162330	-0.111380	3.952049
579.952782	5329.134371	16.167335	-0.111354	3.949157
579.863678	5321.164090	16.172339	-0.111333	3.946277
579.646582	5313.130108	16.177344	-0.111287	3.943370
579.219557	5305.224094	16.182349	-0.111202	3.940504
579.814480	5297.122114	16.187354	-0.111308	3.937583
579.941515	5289.091093	16.192359	-0.111326	3.934677
579.702865	5281.167323	16.197363	-0.111276	3.931801
579.686437	5273.091767	16.202368	-0.111268	3.928872
579.875465	5265.148386	16.207373	-0.111298	3.925992
579.552593	5257.155595	16.212378	-0.111233	3.923083
579.002752	5249.233891	16.217383	-0.111125	3.920194
579.591658	5241.159427	16.222387	-0.111229	3.917268
579.466050	5233.094673	16.227392	-0.111201	3.914330
579.144880	5225.199645	16.232397	-0.111136	3.911447
579.089757	5217.161311	16.237402	-0.111120	3.908516
579.198262	5209.140062	16.242407	-0.111135	3.905591
579.124508	5201.200268	16.247411	-0.111116	3.902691
579.155032	5193.153243	16.252416	-0.111117	3.899751
578.938376	5185.203157	16.257421	-0.111071	3.896840
578.463662	5177.224345	16.262426	-0.110977	3.893911
578.242444	5169.230428	16.267431	-0.110931	3.890979
578.507695	5161.171221	16.272435	-0.110975	3.888031
578.377415	5153.183716	16.277440	-0.110945	3.885099
578.496768	5145.206573	16.282445	-0.110962	3.882173
578.817067	5137.138615	16.287450	-0.111017	3.879216
578.743248	5129.232415	16.292455	-0.110998	3.876308
578.736191	5121.158850	16.297459	-0.110991	3.873338
578.333886	5113.091267	16.302464	-0.110911	3.870359
578.314607	5105.126590	16.307469	-0.110902	3.867424
578.587067	5097.058658	16.312474	-0.110948	3.864455
578.352228	5089.168886	16.317479	-0.110899	3.861539
578.411820	5081.185038	16.322483	-0.110905	3.858591
577.819019	5073.276849	16.327488	-0.110789	3.855656
578.026604	5065.181326	16.332493	-0.110822	3.852667
577.605735	5057.237997	16.337498	-0.110739	3.849717
577.645568	5049.225934	16.342503	-0.110741	3.846750
577.431415	5041.279123	16.347507	-0.110696	3.843800
577.651168	5033.195114	16.352512	-0.110731	3.840805
578.113853	5025.179879	16.357517	-0.110812	3.837839
577.976193	5017.190068	16.362522	-0.110781	3.834867
577.603798	5009.274615	16.367527	-0.110707	3.831916
578.229406	5001.163394	16.372531	-0.110818	3.828910
578.082241	4993.209598	16.377536	-0.110785	3.825945
578.085711	4985.227301	16.382541	-0.110781	3.822969
577.611464	4977.280006	16.387546	-0.110687	3.819994
577.789716	4969.256512	16.392551	-0.110715	3.817003
577.701767	4961.240714	16.397555	-0.110694	3.814006
577.263518	4953.292855	16.402560	-0.110607	3.811025
576.983971	4945.316986	16.407565	-0.110550	3.808034
576.683780	4937.281242	16.412570	-0.110488	3.805018
576.858359	4929.274470	16.417575	-0.110516	3.802020
576.671748	4921.258124	16.422579	-0.110476	3.799009
576.732515	4913.283244	16.427584	-0.110482	3.796017
576.680545	4905.302321	16.432589	-0.110467	3.793017
576.856848	4897.191933	16.437594	-0.110494	3.789972
576.633859	4889.254851	16.442599	-0.110448	3.786980
576.963429	4881.202691	16.447603	-0.110504	3.783955
576.719272	4873.280443	16.452608	-0.110453	3.780963
576.699912	4865.278836	16.457613	-0.110444	3.777945
576.998879	4857.227714	16.462618	-0.110494	3.774912
577.064419	4849.221274	16.467623	-0.110501	3.771889
576.786866	4841.274625	16.472627	-0.110445	3.768878
576.764134	4833.263401	16.477632	-0.110435	3.765846
576.589927	4825.356237	16.482637	-0.110397	3.762847
576.352893	4817.330110	16.487642	-0.110348	3.759799
576.694427	4809.287558	16.492647	-0.110406	3.756757
576.890662	4801.261321	16.497651	-0.110438	3.753714
576.753319	4793.285514	16.502656	-0.110407	3.750681
576.585849	4785.324696	16.507661	-0.110370	3.747650
576.966953	4777.249539	16.512666	-0.110436	3.744586
577.037180	4769.311201	16.517671	-0.110444	3.741564
576.870151	4761.328879	16.522675	-0.110408	3.738517
576.506013	4753.374744	16.527680	-0.110335	3.735474
576.481907	4745.411990	16.532685	-0.110325	3.732433
576.340245	4737.322834	16.537690	-0.110293	3.729338
576.073274	4729.406852	16.542695	-0.110238	3.726304
576.399241	4721.366120	16.547699	-0.110294	3.723235
575.881892	4713.412690	16.552704	-0.110192	3.720175
576.188396	4705.393680	16.557709	-0.110244	3.717109
575.950513	4697.355707	16.562714	-0.110194	3.714018
575.651878	4689.399214	16.567719	-0.110133	3.710955
576.000963	4681.310258	16.572723	-0.110193	3.707855
576.093306	4673.265927	16.577728	-0.110205	3.704763
575.738851	4665.434512	16.582733	-0.110134	3.701739
574.886737	4657.466881	16.587738	-0.109970	3.698648
575.618410	4649.351668	16.592743	-0.110101	3.695537
575.917266	4641.347017	16.597747	-0.110151	3.692455
575.120082	4633.389071	16.602752	-0.109998	3.689360
574.547384	4625.515940	16.607757	-0.109886	3.686302
574.475900	4617.451371	16.612762	-0.109867	3.683180
575.267031	4609.339533	16.617767	-0.110009	3.680059
574.799346	4601.463490	16.622771	-0.109917	3.676994
574.810717	4593.394403	16.627776	-0.109914	3.673864
575.030262	4585.429760	16.632781	-0.109949	3.670778
574.433623	4577.465559	16.637786	-0.109833	3.667667
574.450540	4569.428700	16.642791	-0.109831	3.664542
574.709116	4561.450266	16.647795	-0.109874	3.661444
574.671659	4553.409923	16.652800	-0.109862	3.658310
574.317197	4545.490406	16.657805	-0.109790	3.655213
574.349427	4537.479839	16.662810	-0.109791	3.652088
574.758142	4529.360512	16.667815	-0.109862	3.648928
574.166497	4521.526001	16.672819	-0.109747	3.645849
574.211313	4513.482480	16.677824	-0.109750	3.642703
574.700797	4505.415580	16.682829	-0.109836	3.639558
574.673873	4497.479259	16.687834	-0.109825	3.636447
574.233162	4489.531120	16.692839	-0.109738	3.633317
574.443573	4481.496409	16.697843	-0.109772	3.630169
574.320756	4473.487387	16.702848	-0.109744	3.627018
574.513775	4465.451873	16.707853	-0.109774	3.623863
573.786609	4457.594167	16.712858	-0.109634	3.620750
573.820678	4449.552224	16.717863	-0.109635	3.617583
573.885608	4441.540433	16.722867	-0.109642	3.614426
574.253992	4433.446647	16.727872	-0.109705	3.611242
574.342750	4425.483439	16.732877	-0.109716	3.608099
573.964238	4417.518987	16.737882	-0.109641	3.604939
573.586494	4409.605015	16.742887	-0.109565	3.601797
573.567042	4401.599662	16.747891	-0.109556	3.598626
573.717107	4393.560719	16.752896	-0.109579	3.595444
573.986380	4385.535089	16.757901	-0.109624	3.592267
574.061380	4377.505488	16.762906	-0.109633	3.589081
573.890886	4369.525315	16.767911	-0.109596	3.585905
573.753568	4361.587513	16.772915	-0.109565	3.582743
573.323409	4353.633678	16.777920	-0.109479	3.579563
573.467252	4345.665868	16.782925	-0.109501	3.576392
573.541394	4337.581916	16.787930	-0.109509	3.573170
573.829542	4329.522954	16.792935	-0.109558	3.569961
574.185579	4321.513700	16.797939	-0.109619	3.566772
574.065335	4313.532948	16.802944	-0.109591	3.563576
574.062780	4305.625449	16.807949	-0.109586	3.560411
573.359184	4297.710585	16.812954	-0.109449	3.557219
573.329953	4289.669955	16.817959	-0.109439	3.553993
573.477109	4281.593802	16.822963	-0.109461	3.550756
573.403491	4273.585139	16.827968	-0.109442	3.547536
573.415243	4265.602149	16.832973	-0.109439	3.544327
573.317155	4257.638612	16.837978	-0.109415	3.541118
572.559670	4249.745737	16.842983	-0.109269	3.537916
572.505846	4241.710661	16.847987	-0.109254	3.534674
572.475712	4233.703595	16.852992	-0.109243	3.531441
572.418545	4225.725267	16.857997	-0.109227	3.528217
572.125798	4217.703705	16.863002	-0.109167	3.524964
572.066851	4209.754924	16.868007	-0.109151	3.521745
571.835041	4201.778280	16.873011	-0.109103	3.518507
571.993684	4193.668760	16.878016	-0.109127	3.515224
572.448280	4185.689072	16.883021	-0.109206	3.512000
572.439246	4177.656606	16.888026	-0.109199	3.508737
572.526707	4169.644807	16.893031	-0.109210	3.505482
572.669217	4161.698215	16.898035	-0.109232	3.502253
572.403263	4153.701324	16.903040	-0.109177	3.498987
572.373333	4145.770755	16.908045	-0.109166	3.495752
571.842453	4137.806011	16.913050	-0.109062	3.492485
572.064085	4129.739041	16.918055	-0.109098	3.489197
572.010865	4121.770819	16.923059	-0.109083	3.485937
571.731458	4113.770107	16.928064	-0.109026	3.482654
572.105681	4105.729573	16.933069	-0.109090	3.479372
572.270458	4097.768740	16.938074	-0.109115	3.476113
572.310855	4089.775076	16.943079	-0.109118	3.472834
572.339579	4081.778491	16.948083	-0.109118	3.469550
572.079947	4073.801280	16.953088	-0.109064	3.466261
572.281372	4065.774119	16.958093	-0.109096	3.462964
572.366410	4057.751044	16.963098	-0.109107	3.459662
572.240391	4049.818532	16.968103	-0.109078	3.456386
572.120815	4041.826549	16.973107	-0.109051	3.453084
571.957196	4033.813382	16.978112	-0.109015	3.449767
572.275465	4025.801124	16.983117	-0.109069	3.446465
572.178883	4017.826568	16.988122	-0.109046	3.443160
572.007326	4009.865864	16.993127	-0.109009	3.439856
571.856603	4001.940524	16.998131	-0.108975	3.436564
571.786165	3993.921532	17.003136	-0.108957	3.433232
571.723362	3985.921745	17.008141	-0.108940	3.429906
571.732919	3977.907261	17.013146	-0.108937	3.426572
571.448564	3969.942945	17.018151	-0.108878	3.423247
571.535577	3961.954130	17.023155	-0.108889	3.419920
571.272142	3953.985804	17.028160	-0.108835	3.416587
571.488682	3945.936714	17.033165	-0.108870	3.413233
571.533421	3937.900118	17.038170	-0.108873	3.409875
571.059527	3930.001463	17.043175	-0.108780	3.406554
570.697580	3922.035011	17.048179	-0.108707	3.403205
571.000326	3913.981826	17.053184	-0.108758	3.399839
570.687447	3906.068069	17.058189	-0.108695	3.396507
570.839836	3897.963848	17.063194	-0.108718	3.393108
570.441502	3889.989392	17.068199	-0.108638	3.389741
570.640151	3881.976698	17.073203	-0.108670	3.386375
570.475483	3873.948803	17.078208	-0.108634	3.382987
570.329717	3866.044319	17.083213	-0.108602	3.379648
570.637742	3857.995011	17.088218	-0.108654	3.376261
570.883138	3849.964925	17.093223	-0.108694	3.372876
570.633243	3842.005332	17.098227	-0.108643	3.369500
570.436476	3834.031570	17.103232	-0.108601	3.366116
569.986591	3826.144493	17.108237	-0.108512	3.362757
569.532337	3818.158521	17.113242	-0.108422	3.359352
569.283504	3810.210047	17.118247	-0.108370	3.355966
569.500186	3802.135255	17.123251	-0.108405	3.352541
569.384687	3794.101260	17.128256	-0.108379	3.349118
569.070753	3786.189568	17.133261	-0.108315	3.345735
569.421096	3778.100513	17.138266	-0.108375	3.342299
569.146519	3770.157087	17.143271	-0.108319	3.338897
569.461526	3762.118889	17.148275	-0.108372	3.335474
569.234434	3754.156307	17.153280	-0.108324	3.332059
569.534432	3746.124803	17.158285	-0.108375	3.328631
568.971305	3738.196825	17.163290	-0.108265	3.325211
569.049998	3730.234835	17.168295	-0.108274	3.321798
569.357839	3722.193050	17.173299	-0.108326	3.318355
569.240899	3714.196620	17.178304	-0.108299	3.314912
569.242432	3706.213918	17.183309	-0.108294	3.311476
568.823902	3698.245988	17.188314	-0.108211	3.308027
568.742135	3690.230306	17.193319	-0.108191	3.304566
569.100416	3682.253579	17.198323	-0.108252	3.301135
568.992507	3674.221603	17.203328	-0.108227	3.297659
569.257149	3666.186852	17.208333	-0.108271	3.294193
569.187995	3658.220188	17.213338	-0.108253	3.290739
568.640176	3650.319743	17.218343	-0.108146	3.287292
568.863707	3642.249179	17.223347	-0.108182	3.283798
568.553193	3634.333418	17.228352	-0.108119	3.280346
568.548672	3626.373816	17.233357	-0.108113	3.276883
568.259929	3618.390597	17.238362	-0.108054	3.273395
568.450283	3610.352775	17.243367	-0.108084	3.269899
568.283007	3602.381349	17.248371	-0.108048	3.266413
567.639279	3594.442390	17.253376	-0.107923	3.262919
568.114049	3586.372653	17.258381	-0.108006	3.259409
568.053212	3578.395120	17.263386	-0.107989	3.255914
568.180388	3570.383846	17.268391	-0.108007	3.252408
568.870980	3562.269095	17.273395	-0.108131	3.248876
568.803394	3554.333554	17.278400	-0.108113	3.245388
568.654906	3546.413416	17.283405	-0.108080	3.241899
568.096501	3538.498355	17.288410	-0.107971	3.238392
567.900661	3530.529165	17.293415	-0.107929	3.234872
567.519028	3522.588302	17.298419	-0.107853	3.231354
567.615333	3514.489817	17.303424	-0.107866	3.227781
567.400355	3506.509333	17.308429	-0.107820	3.224244
567.736037	3498.477268	17.313434	-0.107878	3.220703
567.146216	3490.571009	17.318439	-0.107763	3.217175
567.088919	3482.555000	17.323443	-0.107747	3.213617
566.893315	3474.548391	17.328448	-0.107705	3.210053
566.816489	3466.573157	17.333453	-0.107685	3.206504
566.898826	3458.543237	17.338458	-0.107695	3.202934
566.958129	3450.567154	17.343463	-0.107701	3.199383
566.960182	3442.600486	17.348467	-0.107696	3.195829
566.928224	3434.560699	17.353472	-0.107685	3.192238
567.021215	3426.585666	17.358477	-0.107697	3.188676
567.281268	3418.529502	17.363482	-0.107740	3.185082
567.012360	3410.598140	17.368487	-0.107685	3.181517
566.950486	3402.647429	17.373491	-0.107668	3.177948
567.084467	3394.592897	17.378496	-0.107688	3.174336
567.015497	3386.663651	17.383501	-0.107670	3.170769
566.841942	3378.689765	17.388506	-0.107632	3.167172
566.756312	3370.699834	17.393511	-0.107611	3.163568
566.242050	3362.777533	17.398515	-0.107510	3.159972
566.043837	3354.797645	17.403520	-0.107468	3.156359
566.346419	3346.731635	17.408525	-0.107519	3.152725
566.455588	3338.715153	17.413530	-0.107534	3.149101
566.169877	3330.763950	17.418535	-0.107476	3.145485
566.293584	3322.770632	17.423539	-0.107494	3.141864
566.132152	3314.791309	17.428544	-0.107458	3.138232
565.748505	3306.857042	17.433549	-0.107382	3.134606
565.591534	3298.860310	17.438554	-0.107347	3.130958
565.790975	3290.816313	17.443559	-0.107379	3.127300
565.842353	3282.814161	17.448563	-0.107383	3.123651
565.443498	3274.883361	17.453568	-0.107304	3.120009
565.504729	3266.910544	17.458573	-0.107310	3.116365
565.724712	3258.865709	17.463578	-0.107346	3.112690
565.153215	3250.933564	17.468583	-0.107234	3.109027
565.194248	3242.937875	17.473587	-0.107236	3.105358
564.973520	3234.968500	17.478592	-0.107190	3.101685
565.100060	3226.959365	17.483597	-0.107208	3.098006
564.504341	3219.031422	17.488602	-0.107092	3.094325
564.875332	3210.956347	17.493607	-0.107156	3.090618
564.609422	3203.036551	17.498611	-0.107101	3.086948
564.342794	3195.022462	17.503616	-0.107046	3.083230
564.394664	3187.044337	17.508621	-0.107051	3.079539
565.169403	3178.960160	17.513626	-0.107190	3.075829
564.701408	3171.007847	17.518631	-0.107097	3.072117
564.912160	3162.965557	17.523635	-0.107131	3.068390
565.086247	3154.949443	17.528640	-0.107159	3.064670
565.157335	3147.034643	17.533645	-0.107167	3.060987
564.845952	3139.097852	17.538650	-0.107103	3.057271
564.610373	3131.134969	17.543655	-0.107054	3.053542
564.527047	3123.145483	17.548659	-0.107034	3.049804
564.226344	3115.166384	17.553664	-0.106972	3.046055
564.436911	3107.146801	17.558669	-0.107006	3.042307
564.786331	3099.111898	17.563674	-0.107066	3.038555
563.712935	3091.312190	17.568679	-0.106861	3.034838
563.715539	3083.307993	17.573683	-0.106856	3.031074
563.782659	3075.239408	17.578688	-0.106864	3.027277
563.930542	3067.239935	17.583693	-0.106886	3.023513
563.961835	3059.242774	17.588698	-0.106886	3.019739
564.326973	3051.223093	17.593703	-0.106949	3.015966
564.228368	3043.272714	17.598707	-0.106926	3.012199
564.221556	3035.248894	17.603712	-0.106919	3.008396
564.375554	3027.283962	17.608717	-0.106942	3.004625
563.791624	3019.445951	17.613722	-0.106829	3.000872
563.915746	3011.378847	17.618727	-0.106846	2.997041
564.097674	3003.353183	17.623731	-0.106875	2.993228
563.605040	2995.434438	17.628736	-0.106778	2.989426
563.833350	2987.390860	17.633741	-0.106815	2.985597
563.860363	2979.403823	17.638746	-0.106815	2.981780
563.641284	2971.442304	17.643751	-0.106769	2.977957
564.107463	2963.371964	17.648755	-0.106851	2.974113
563.840923	2955.422504	17.653760	-0.106796	2.970284
563.816867	2947.490410	17.658765	-0.106786	2.966470
563.948968	2939.493961	17.663770	-0.106805	2.962629
563.382709	2931.592422	17.668775	-0.106695	2.958793
563.130501	2923.664813	17.673779	-0.106643	2.954955
563.329500	2915.582403	17.678784	-0.106674	2.951061
563.337017	2907.596524	17.683789	-0.106670	2.947198
563.939782	2899.484760	17.688794	-0.106777	2.943301
564.200308	2891.488320	17.693799	-0.106821	2.939437
563.923666	2883.640653	17.698803	-0.106764	2.935611
563.738297	2875.658627	17.703808	-0.106724	2.931720
563.814020	2867.647118	17.708813	-0.106733	2.927823
563.678418	2859.712976	17.713818	-0.106703	2.923947
563.089297	2851.816356	17.718823	-0.106588	2.920060
563.405167	2843.786071	17.723827	-0.106641	2.916152
563.069149	2835.761935	17.728832	-0.106573	2.912205
563.379491	2827.739049	17.733837	-0.106626	2.908289
563.552509	2819.684188	17.738842	-0.106653	2.904345
563.782531	2811.720172	17.743847	-0.106690	2.900443
563.888037	2803.762222	17.748851	-0.106705	2.896532
563.672800	2795.810832	17.753856	-0.106660	2.892602
563.576195	2787.812869	17.758861	-0.106636	2.888649
562.958844	2779.942861	17.763866	-0.106516	2.884726
563.025754	2771.949225	17.768871	-0.106523	2.880774
563.164055	2763.947808	17.773875	-0.106544	2.876816
563.149080	2755.936209	17.778880	-0.106536	2.872840
563.110581	2747.983563	17.783885	-0.106523	2.868886
563.008411	2739.988897	17.788890	-0.106499	2.864902
562.562063	2732.079365	17.793895	-0.106411	2.860935
563.055071	2724.008431	17.798899	-0.106497	2.856936
563.149483	2716.001848	17.803904	-0.106510	2.852940
562.692728	2708.101457	17.808909	-0.106420	2.848961
563.024912	2700.050986	17.813914	-0.106476	2.844946
562.733672	2692.137466	17.818919	-0.106417	2.840958
563.008025	2684.142703	17.823923	-0.106462	2.836956
562.920063	2676.145330	17.828928	-0.106441	2.832926
563.089357	2668.166439	17.833933	-0.106467	2.828915
562.904159	2660.195557	17.838938	-0.106427	2.824882
562.816657	2652.231722	17.843943	-0.106406	2.820852
563.009107	2644.223657	17.848947	-0.106436	2.816810
562.491269	2636.335366	17.853952	-0.106335	2.812782
562.283202	2628.356493	17.858957	-0.106291	2.808720
562.536889	2620.307609	17.863962	-0.106333	2.804644
561.860402	2612.446747	17.868967	-0.106202	2.800602
562.000282	2604.443458	17.873971	-0.106223	2.796530
562.289684	2596.355528	17.878976	-0.106271	2.792418
562.504597	2588.381993	17.883981	-0.106306	2.788355
562.454499	2580.389957	17.888986	-0.106291	2.784259
562.122197	2572.501704	17.893991	-0.106224	2.780195
562.026546	2564.530641	17.898995	-0.106201	2.776095
561.718803	2556.556848	17.904000	-0.106139	2.771976
561.838429	2548.546696	17.909005	-0.106156	2.767857
561.556587	2540.598053	17.914010	-0.106098	2.763740
561.771007	2532.600512	17.919015	-0.106133	2.759621
561.590451	2524.665634	17.924019	-0.106094	2.755505
561.085321	2516.694391	17.929024	-0.105995	2.751344
561.323476	2508.652274	17.934029	-0.106034	2.747185
560.929801	2500.723560	17.939034	-0.105955	2.743040
560.974242	2492.712443	17.944039	-0.105958	2.738873
561.184754	2484.723647	17.949043	-0.105992	2.734721
560.939248	2476.752825	17.954048	-0.105941	2.730544
560.948769	2468.778204	17.959053	-0.105938	2.726375
560.687078	2460.850593	17.964058	-0.105884	2.722206
560.296280	2452.908509	17.969063	-0.105806	2.718016
560.166681	2444.951118	17.974067	-0.105776	2.713828
560.079666	2436.922703	17.979072	-0.105755	2.709598
560.043785	2428.955771	17.984077	-0.105743	2.705397
560.018196	2420.997625	17.989082	-0.105733	2.701195
560.149911	2412.946720	17.994087	-0.105752	2.696948
560.346979	2404.981826	17.999091	-0.105784	2.692743
559.714152	2397.072139	18.004096	-0.105661	2.688509
559.686372	2389.095991	18.009101	-0.105650	2.684270
560.309112	2381.025833	18.014106	-0.105761	2.680018
560.226909	2373.089645	18.019111	-0.105740	2.675784
559.868553	2365.175177	18.024115	-0.105668	2.671537
559.525848	2357.205056	18.029120	-0.105599	2.667255
559.965695	2349.158049	18.034125	-0.105676	2.662975
559.969488	2341.188186	18.039130	-0.105672	2.658702
559.646773	2333.240409	18.044135	-0.105606	2.654412
560.010315	2325.227714	18.049139	-0.105669	2.650125
559.995764	2317.244486	18.054144	-0.105661	2.645823
559.364305	2309.423123	18.059149	-0.105538	2.641560
558.530757	2301.555453	18.064154	-0.105378	2.637251
558.640070	2293.497836	18.069159	-0.105393	2.632895
559.055077	2285.436903	18.074163	-0.105465	2.628551
558.800263	2277.460652	18.079168	-0.105412	2.624200
558.891593	2269.510947	18.084173	-0.105424	2.619880
558.929113	2261.530917	18.089178	-0.105425	2.615533
559.196780	2253.500024	18.094183	-0.105470	2.611166
559.164215	2245.543831	18.099187	-0.105459	2.606813
558.815293	2237.643625	18.104192	-0.105389	2.602461
558.311468	2229.763441	18.109197	-0.105290	2.598102
558.555056	2221.696078	18.114202	-0.105330	2.593685
558.265423	2213.652627	18.119207	-0.105270	2.589236
558.356629	2205.678760	18.124211	-0.105282	2.584844
558.265766	2197.701802	18.129216	-0.105260	2.580431
558.301519	2189.747647	18.134221	-0.105261	2.576031
558.125684	2181.811568	18.139226	-0.105224	2.571619
558.005112	2173.834752	18.144231	-0.105196	2.567180
557.691500	2165.935799	18.149235	-0.105132	2.562764
557.892952	2157.915852	18.154240	-0.105165	2.558309
557.944727	2149.950011	18.159245	-0.105169	2.553866
557.623046	2142.021286	18.164250	-0.105104	2.549409
557.357144	2134.069157	18.169255	-0.105049	2.544935
557.617283	2126.063426	18.174259	-0.105092	2.540461
557.387818	2118.120112	18.179264	-0.105044	2.535979
557.142576	2110.178598	18.184269	-0.104993	2.531489
558.055991	2102.024706	18.189274	-0.105158	2.526954
557.543606	2094.180120	18.194279	-0.105058	2.522484
557.839526	2086.190917	18.199283	-0.105107	2.517982
557.946634	2078.209352	18.204288	-0.105122	2.513462
557.007213	2070.425728	18.209293	-0.104942	2.508970
556.590931	2062.444065	18.214298	-0.104859	2.504396
556.991431	2054.396108	18.219303	-0.104929	2.499836
557.193275	2046.398983	18.224307	-0.104961	2.495281
556.895582	2038.428059	18.229312	-0.104900	2.490697
556.705299	2030.502896	18.234317	-0.104860	2.486138
556.987398	2022.495301	18.239322	-0.104907	2.481559
556.247932	2014.663994	18.244327	-0.104764	2.476996
556.903605	2006.570680	18.249331	-0.104881	2.472378
557.105003	1998.551221	18.254336	-0.104913	2.467760
557.120167	1990.611184	18.259341	-0.104911	2.463166
556.608630	1982.748861	18.264346	-0.104810	2.458568
556.528771	1974.786860	18.269351	-0.104790	2.453936
555.984203	1966.930288	18.274355	-0.104684	2.449321
556.410570	1958.812495	18.279360	-0.104758	2.444620
556.071117	1950.946158	18.284365	-0.104689	2.439997
556.505367	1942.896509	18.289370	-0.104765	2.435318
556.365335	1934.910668	18.294375	-0.104734	2.430624
555.937871	1927.010283	18.299379	-0.104649	2.425947
555.607465	1919.089204	18.304384	-0.104582	2.421258
555.845844	1911.072643	18.309389	-0.104621	2.416547
555.675016	1903.098064	18.314394	-0.104584	2.411819
556.083576	1895.067768	18.319399	-0.104655	2.407096
556.049659	1887.138582	18.324403	-0.104643	2.402387
555.913210	1879.206928	18.329408	-0.104613	2.397660
556.214194	1871.193159	18.334413	-0.104664	2.392910
555.861203	1863.317537	18.339418	-0.104593	2.388180
555.759018	1855.357054	18.344423	-0.104569	2.383410
555.699403	1847.419588	18.349427	-0.104552	2.378648
555.589625	1839.472605	18.354432	-0.104527	2.373867
555.217062	1831.590092	18.359437	-0.104452	2.369093
554.909468	1823.618725	18.364442	-0.104389	2.364261
555.312785	1815.574144	18.369447	-0.104459	2.359433
555.213093	1807.664878	18.374451	-0.104436	2.354637
554.955668	1799.716072	18.379456	-0.104382	2.349793
554.944471	1791.717795	18.384461	-0.104375	2.344929
554.958760	1783.773341	18.389466	-0.104372	2.340090
555.234603	1775.756795	18.394471	-0.104419	2.335219
555.322485	1767.789302	18.399475	-0.104430	2.330352
554.960864	1759.894192	18.404480	-0.104357	2.325482
555.536657	1751.853858	18.409485	-0.104459	2.320591
555.751846	1743.891126	18.414490	-0.104494	2.315707
555.172193	1736.058877	18.419495	-0.104381	2.310826
555.261382	1728.077267	18.424499	-0.104392	2.305899
555.163156	1720.123073	18.429504	-0.104369	2.300963
554.669905	1712.275833	18.434509	-0.104272	2.296048
555.057630	1704.225197	18.439514	-0.104339	2.291072
555.224110	1696.241841	18.444519	-0.104364	2.286108
554.527091	1688.438818	18.449523	-0.104230	2.281171
554.322240	1680.499075	18.454528	-0.104186	2.276181
554.773487	1672.428473	18.459533	-0.104265	2.271154
554.377416	1664.510965	18.464538	-0.104186	2.266139
554.384538	1656.533145	18.469543	-0.104182	2.261110
554.486734	1648.577827	18.474547	-0.104196	2.256092
554.003761	1640.698114	18.479552	-0.104101	2.251059
553.887821	1632.730294	18.484557	-0.104074	2.245991
553.705065	1624.810458	18.489562	-0.104035	2.240937
553.919529	1616.800386	18.494567	-0.104069	2.235849
554.086968	1608.842548	18.499571	-0.104095	2.230778
553.640940	1600.946482	18.504576	-0.104007	2.225681
553.820911	1592.955982	18.509581	-0.104035	2.220567
553.662042	1585.037528	18.514586	-0.104001	2.215457
553.455969	1577.102757	18.519591	-0.103957	2.210321
553.597691	1569.127069	18.524595	-0.103978	2.205178
553.391005	1561.232620	18.529600	-0.103934	2.200044
553.260537	1553.284001	18.534605	-0.103905	2.194869
553.243416	1545.346513	18.539610	-0.103897	2.189700
553.451597	1537.320031	18.544615	-0.103930	2.184482
553.443904	1529.398555	18.549619	-0.103923	2.179299
553.062705	1521.513187	18.554624	-0.103847	2.174093
553.065904	1513.548510	18.559629	-0.103843	2.168859
553.514956	1505.521165	18.564634	-0.103921	2.163612
553.125937	1497.669587	18.569639	-0.103843	2.158390
553.113728	1489.736001	18.574643	-0.103836	2.153136
553.151358	1481.784320	18.579648	-0.103838	2.147862
552.622772	1473.927775	18.584653	-0.103734	2.142584
552.402682	1466.015762	18.589658	-0.103688	2.137286
552.255167	1458.057105	18.594663	-0.103655	2.131951
552.243061	1450.108715	18.599667	-0.103648	2.126622
552.135200	1442.168073	18.604672	-0.103622	2.121275
552.637938	1434.146780	18.609677	-0.103711	2.115920
552.221906	1426.258258	18.614682	-0.103628	2.110551
552.317762	1418.243177	18.619687	-0.103641	2.105133
552.055167	1410.379181	18.624691	-0.103587	2.099769
551.896816	1402.447704	18.629696	-0.103552	2.094355
551.970355	1394.491221	18.634701	-0.103560	2.088933
552.197506	1386.509018	18.639706	-0.103597	2.083494
552.084722	1378.612723	18.644711	-0.103571	2.078066
552.479933	1370.638678	18.649715	-0.103640	2.072622
551.694912	1362.813544	18.654720	-0.103488	2.067147
551.917880	1354.829204	18.659725	-0.103525	2.061649
552.339655	1346.840414	18.664730	-0.103598	2.056154
551.680566	1339.023917	18.669735	-0.103470	2.050653
551.770350	1331.081663	18.674739	-0.103482	2.045127
551.766312	1323.148717	18.679744	-0.103476	2.039582
551.359996	1315.299062	18.684749	-0.103395	2.034039
551.502133	1307.309404	18.689754	-0.103416	2.028440
551.215696	1299.401243	18.694759	-0.103357	2.022838
551.182978	1291.488459	18.699763	-0.103346	2.017243
551.036151	1283.543035	18.704768	-0.103314	2.011598
551.141863	1275.586050	18.709773	-0.103328	2.005955
550.975295	1267.711916	18.714778	-0.103292	2.000326
550.793018	1259.804580	18.719783	-0.103253	1.994656
550.633460	1251.903629	18.724787	-0.103218	1.988977
550.881043	1243.892407	18.729792	-0.103259	1.983246
551.346833	1235.903104	18.734797	-0.103340	1.977538
551.117156	1228.035694	18.739802	-0.103292	1.971826
551.631067	1220.010474	18.744807	-0.103383	1.966064
551.623440	1212.144816	18.749811	-0.103376	1.960344
551.157036	1204.321992	18.754816	-0.103284	1.954589
551.279571	1196.393997	18.759821	-0.103302	1.948804
551.287460	1188.451624	18.764826	-0.103298	1.942979
550.884964	1180.603121	18.769831	-0.103218	1.937160
550.615244	1172.723838	18.774835	-0.103162	1.931315
550.208353	1164.843839	18.779840	-0.103082	1.925437
550.229398	1156.915099	18.784845	-0.103080	1.919552
549.867797	1149.044499	18.789850	-0.103008	1.913650
550.430606	1140.986116	18.794855	-0.103107	1.907693
549.985011	1133.175763	18.799859	-0.103019	1.901789
549.983485	1125.243729	18.804864	-0.103014	1.895826
549.747537	1117.341501	18.809869	-0.102965	1.889839
550.203291	1109.345478	18.814874	-0.103044	1.883843
550.009439	1101.482018	18.819879	-0.103003	1.877852
549.955650	1093.571415	18.824883	-0.102988	1.871823
549.890161	1085.650761	18.829888	-0.102970	1.865765
549.525702	1077.818111	18.834893	-0.102897	1.859720
549.478903	1069.901486	18.839898	-0.102883	1.853628
549.312970	1061.995644	18.844903	-0.102847	1.847510
549.587534	1054.060059	18.849907	-0.102893	1.841401
549.359616	1046.198966	18.854912	-0.102846	1.835270
548.547973	1038.434862	18.859917	-0.102689	1.829123
548.891307	1030.432218	18.864922	-0.102748	1.822908
548.827186	1022.524625	18.869927	-0.102731	1.816697
548.720906	1014.626457	18.874931	-0.102706	1.810468
549.009948	1006.671218	18.879936	-0.102755	1.804220
549.069024	998.789897	18.884941	-0.102760	1.797980
548.827728	990.933488	18.889946	-0.102710	1.791702
548.685267	983.013095	18.894951	-0.102679	1.785363
548.662077	975.132898	18.899955	-0.102669	1.779048
548.481433	967.253241	18.904960	-0.102630	1.772691
548.759448	959.304718	18.909965	-0.102677	1.766313
548.511985	951.473801	18.914970	-0.102626	1.759942
548.695411	943.558972	18.919975	-0.102655	1.753533
548.627191	935.684941	18.924979	-0.102637	1.747103
548.381399	927.840537	18.929984	-0.102586	1.740650
548.227134	919.999282	18.934989	-0.102552	1.734187
547.927946	912.155912	18.939994	-0.102491	1.727679
547.643691	904.297636	18.944999	-0.102433	1.721137
547.637108	896.418404	18.950003	-0.102427	1.714588
547.708772	888.488527	18.955008	-0.102435	1.707982
547.686153	880.594975	18.960013	-0.102425	1.701369
547.859100	872.695041	18.965018	-0.102452	1.694750
547.863335	864.808515	18.970023	-0.102448	1.688094
548.256381	856.884414	18.975027	-0.102516	1.681433
547.262262	849.204076	18.980032	-0.102326	1.674765
547.353359	841.306054	18.985037	-0.102337	1.668031
547.458870	833.406778	18.990042	-0.102352	1.661271
547.290774	825.549592	18.995047	-0.102315	1.654482
547.450623	817.664364	19.000051	-0.102340	1.647686
546.980278	809.889621	19.005056	-0.102247	1.640870
546.973552	802.021148	19.010061	-0.102241	1.634009
547.110722	794.088446	19.015066	-0.102261	1.627083
546.950544	786.244567	19.020071	-0.102226	1.620163
546.794693	778.422314	19.025075	-0.102192	1.613234
546.944214	770.508850	19.030080	-0.102215	1.606237
547.090822	762.648985	19.035085	-0.102237	1.599257
546.644969	754.897516	19.040090	-0.102149	1.592257
546.197607	747.098278	19.045095	-0.102060	1.585184
546.437837	739.211578	19.050099	-0.102100	1.578100
545.990637	731.426003	19.055104	-0.102012	1.570975
545.898402	723.586605	19.060109	-0.101989	1.563821
545.985953	715.728799	19.065114	-0.102000	1.556644
545.925851	707.885419	19.070119	-0.101984	1.549424
545.552227	700.111426	19.075123	-0.101909	1.542188
545.500540	692.259176	19.080128	-0.101895	1.534894
545.565633	684.395496	19.085133	-0.101902	1.527572
545.235220	676.626131	19.090138	-0.101835	1.520242
544.965388	668.838829	19.095143	-0.101780	1.512870
545.090814	660.968062	19.100147	-0.101798	1.505443
544.884301	653.174099	19.105152	-0.101754	1.498001
545.077583	645.302745	19.110157	-0.101785	1.490510
544.894132	637.521326	19.115162	-0.101746	1.483009
544.725577	629.735658	19.120167	-0.101709	1.475467
544.660945	621.899329	19.125171	-0.101692	1.467855
544.232323	614.134890	19.130176	-0.101607	1.460214
544.565673	606.260372	19.135181	-0.101664	1.452548
544.295589	598.499953	19.140186	-0.101609	1.444856
544.063611	590.750763	19.145191	-0.101560	1.437140
543.795854	582.999426	19.150195	-0.101505	1.429374
543.804563	575.167171	19.155200	-0.101502	1.421530
543.782873	567.382428	19.160205	-0.101493	1.413686
544.042465	559.532858	19.165210	-0.101536	1.405779
543.573661	551.841726	19.170215	-0.101444	1.397866
543.534069	544.066810	19.175219	-0.101431	1.389895
543.356432	536.300907	19.180224	-0.101393	1.381864
542.956477	528.594889	19.185229	-0.101313	1.373809
543.282963	520.735006	19.190234	-0.101369	1.365673
543.009374	513.018240	19.195239	-0.101313	1.357533
543.143264	505.229324	19.200243	-0.101333	1.349339
542.676502	497.553308	19.205248	-0.101241	1.341109
542.994932	489.734954	19.210253	-0.101295	1.332816
542.624138	482.050421	19.215258	-0.101221	1.324491
542.379044	474.351182	19.220263	-0.101170	1.316120
542.524041	466.487626	19.225267	-0.101192	1.307587
542.428540	458.757995	19.230272	-0.101169	1.299102
542.512824	451.010053	19.235277	-0.101180	1.290573
542.224863	443.342484	19.240282	-0.101121	1.282008
542.218382	435.613626	19.245287	-0.101115	1.273369
542.067056	427.920450	19.250291	-0.101082	1.264684
542.041811	420.223144	19.255296	-0.101072	1.255958
541.890561	412.538406	19.260301	-0.101039	1.247162
541.689544	404.880419	19.265306	-0.100996	1.238324
541.397859	397.229032	19.270311	-0.100937	1.229412
541.610831	389.495565	19.275315	-0.100971	1.220439
541.104151	381.892183	19.280320	-0.100872	1.211408
541.119112	374.204732	19.285325	-0.100870	1.202316
541.557664	366.452845	19.290330	-0.100946	1.193163
541.320200	358.833901	19.295335	-0.100897	1.183961
541.336192	351.181306	19.300339	-0.100895	1.174698
541.323298	343.533030	19.305344	-0.100888	1.165362
540.965932	335.979377	19.310349	-0.100816	1.155993
540.865668	328.338180	19.315354	-0.100793	1.146494
540.486289	320.771368	19.320359	-0.100717	1.136949
540.523862	313.135482	19.325363	-0.100719	1.127326
539.982989	305.615797	19.330368	-0.100613	1.117641
540.052646	297.990027	19.335373	-0.100621	1.107870
540.064638	290.387435	19.340378	-0.100618	1.098030
539.703890	282.856868	19.345383	-0.100546	1.088111
539.686621	275.290970	19.350387	-0.100538	1.078132
539.414769	267.766369	19.355392	-0.100483	1.068056
539.323837	260.213385	19.360397	-0.100461	1.057888
539.179769	252.677168	19.365402	-0.100429	1.047631
539.111346	245.160515	19.370407	-0.100411	1.037318
539.058374	237.645309	19.375411	-0.100396	1.026907
538.536211	230.229042	19.380416	-0.100294	1.016414
538.338701	222.752032	19.385421	-0.100253	1.005805
538.548034	215.235006	19.390426	-0.100287	0.995128
538.356559	207.755162	19.395431	-0.100246	0.984287
538.095637	200.341507	19.400435	-0.100193	0.973404
538.188463	192.862631	19.405440	-0.100205	0.962393
538.085506	185.451897	19.410445	-0.100181	0.951306
538.000785	178.055655	19.415450	-0.100160	0.940115
538.062616	170.629851	19.420455	-0.100167	0.928782
537.946245	163.294369	19.425459	-0.100141	0.917402
537.707597	155.968793	19.430464	-0.100091	0.905861
537.795156	148.602488	19.435469	-0.100103	0.894197
537.155429	141.406628	19.440474	-0.099979	0.882447
536.546459	134.210991	19.445479	-0.099861	0.870548
536.515643	126.922548	19.450483	-0.099850	0.858499
536.272097	119.694214	19.455488	-0.099800	0.846317
536.257573	112.451919	19.460493	-0.099793	0.834001
535.701714	105.321408	19.465498	-0.099685	0.821529
535.367319	98.165691	19.470503	-0.099618	0.808889
535.275352	91.013503	19.475507	-0.099596	0.796131
534.757960	83.955536	19.480512	-0.099495	0.783200
533.836265	77.005517	19.485517	-0.099319	0.770119
533.501099	70.160158	19.490522	-0.099252	0.757205